Thu Jun 16 10:39:50 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.533285	95.190508	0.000000
0.618578	89.141255	0.005005
0.639421	83.242447	0.010010
0.391161	90.269800	0.015014
0.268446	86.418890	0.020019
0.598790	87.579983	0.025024
0.011102	74.072065	0.030029
0.103811	66.696876	0.035034
-0.027717	60.853544	0.040038
-0.510397	60.552089	0.045043
-0.579897	34.894351	0.050048
-0.922593	40.516287	0.055053
-1.342249	18.253290	0.060058
-1.520331	21.890836	0.065062
-2.011278	16.859641	0.070067
-1.976079	0.076760	0.075072
-2.639394	21.250662	0.080077
-3.088260	4.890690	0.085082
-3.539985	5.650857	0.090086
-3.861480	4.094044	0.095091
-3.508264	-2.240557	0.100096
-3.920225	11.158781	0.105101
-4.206356	-1.462686	0.110106
-4.856701	0.711151	0.115110
-5.530380	-0.434974	0.120115
-5.048379	-0.192352	0.125120
-5.152212	-0.359500	0.130125
-5.167197	-7.278639	0.135130
-5.389246	11.197171	0.140134
-5.847140	4.051513	0.145139
-6.324462	-4.023597	0.150144
-6.702511	12.027158	0.155149
-6.676630	2.968085	0.160154
-6.621542	7.195120	0.165158
-7.093282	8.567284	0.170163
-7.755286	-0.666175	0.175168
-8.430850	2.978898	0.180173
-8.196180	-3.084053	0.185178
-8.214625	8.665193	0.190182
-8.319098	1.480171	0.195187
-8.196466	3.101863	0.200192
-9.172217	3.822945	0.205197
-9.372476	4.954222	0.210202
-9.534399	-0.534930	0.215206
-9.709153	3.507723	0.220211
-9.541156	4.160840	0.225216
-10.570655	7.695412	0.230221
-11.060040	7.688166	0.235226
-11.304299	3.885282	0.240230
-11.199641	11.001664	0.245235
-11.057857	1.182949	0.250240
-11.492536	2.999537	0.255245
-11.209270	9.286622	0.260250
-11.747010	6.790853	0.265254
-12.680397	5.047883	0.270259
-12.455532	-3.109233	0.275264
-13.353323	13.143232	0.280269
-13.205883	6.260680	0.285274
-13.087920	5.041245	0.290278
-13.021032	9.926812	0.295283
-14.057762	6.229733	0.300288
-14.480460	17.394780	0.305293
-14.851695	11.000643	0.310298
-14.898379	9.599667	0.315302
-15.201874	11.808328	0.320307
-14.974025	6.475941	0.325312
-15.062277	11.478401	0.330317
-14.960996	8.683570	0.335322
-15.758937	1.846562	0.340326
-15.983880	11.620867	0.345331
-16.154913	7.797495	0.350336
-16.352680	9.959285	0.355341
-16.850564	12.626647	0.360346
-17.342755	6.989143	0.365350
-17.992436	11.431300	0.370355
-17.895998	-3.527536	0.375360
-17.886869	6.720684	0.380365
-18.048414	8.981652	0.385370
-18.050517	-4.346835	0.390374
-18.320048	9.379279	0.395379
-18.757310	1.073803	0.400384
-19.218128	5.445779	0.405389
-19.223375	1.355976	0.410394
-19.400793	9.130029	0.415398
-19.345707	9.518474	0.420403
-19.801569	0.310733	0.425408
-20.664955	2.849476	0.430413
-20.740440	5.454332	0.435418
-20.820044	11.421274	0.440422
-20.993061	8.694266	0.445427
-20.858055	7.855578	0.450432
-21.549127	14.939107	0.455437
-22.134808	3.302473	0.460442
-22.373711	1.638292	0.465446
-23.111968	7.345316	0.470451
-22.535800	2.598388	0.475456
-22.985640	0.581163	0.480461
-23.023422	3.595215	0.485466
-23.034413	6.929606	0.490470
-23.435164	6.929023	0.495475
-23.562994	0.307027	0.500480
-23.917732	7.304092	0.505485
-24.186955	11.308198	0.510490
-25.017746	3.488808	0.515494
-25.386704	11.579721	0.520499
-25.064186	12.696029	0.525504
-25.945708	11.430060	0.530509
-26.002534	10.377328	0.535514
-25.786112	9.232482	0.540518
-26.216580	10.798882	0.545523
-26.056126	16.783176	0.550528
-26.008837	14.599543	0.555533
-26.394705	2.287461	0.560538
-27.027246	-0.011314	0.565542
-27.555919	14.194267	0.570547
-27.472087	9.060395	0.575552
-27.948090	16.658866	0.580557
-27.948276	7.139346	0.585562
-28.679978	6.788189	0.590566
-29.489510	6.104116	0.595571
-29.238126	6.636118	0.600576
-29.435132	5.110920	0.605581
-29.150099	4.519425	0.610586
-29.424232	2.230871	0.615590
-29.648868	10.607506	0.620595
-29.251644	-2.077264	0.625600
-29.970153	7.955884	0.630605
-30.549497	12.651203	0.635610
-30.834868	1.505365	0.640614
-31.082399	8.136665	0.645619
-31.640217	5.473645	0.650624
-31.739681	5.423173	0.655629
-31.881539	5.682078	0.660634
-31.910838	3.196697	0.665638
-32.170350	17.756653	0.670643
-31.907189	2.993414	0.675648
-33.084469	2.118748	0.680653
-33.165904	5.755214	0.685658
-33.433146	9.017319	0.690662
-33.513066	7.163495	0.695667
-33.794646	4.343544	0.700672
-34.719303	4.261142	0.705677
-34.654572	2.172986	0.710682
-34.795387	-0.103269	0.715686
-35.128235	12.435564	0.720691
-35.147200	-8.902236	0.725696
-35.655547	2.349266	0.730701
-35.372622	2.060786	0.735706
-35.354128	11.220501	0.740710
-35.801343	5.916018	0.745715
-36.502766	11.516332	0.750720
-36.780973	8.068488	0.755725
-36.902183	6.772958	0.760730
-36.742826	2.578411	0.765734
-37.492335	6.891750	0.770739
-37.627001	12.242529	0.775744
-38.406140	11.278093	0.780749
-38.656360	5.699750	0.785754
-38.648846	4.649310	0.790758
-38.585764	5.057841	0.795763
-38.462928	0.264784	0.800768
-38.629016	12.315052	0.805773
-38.971466	2.659233	0.810778
-39.698829	10.506413	0.815782
-40.168958	8.298885	0.820787
-40.114903	2.888676	0.825792
-40.518101	7.616148	0.830797
-40.451348	4.699071	0.835802
-40.828713	10.875828	0.840806
-41.527798	15.519710	0.845811
-41.397201	-2.951786	0.850816
-41.447925	9.448869	0.855821
-41.593639	12.367802	0.860826
-41.772581	1.711552	0.865830
-42.762591	12.185466	0.870835
-42.946971	1.141126	0.875840
-43.073490	3.101826	0.880845
-43.143339	4.212833	0.885850
-43.007932	1.142055	0.890854
-43.205812	3.841028	0.895859
-43.581699	-3.718113	0.900864
-44.290724	15.685801	0.905869
-44.518507	2.333246	0.910874
-44.475130	10.542963	0.915878
-44.628538	0.512986	0.920883
-45.168750	-4.788947	0.925888
-46.071767	-1.451963	0.930893
-46.348668	-0.462707	0.935898
-46.299256	4.034684	0.940902
-46.307353	2.027621	0.945907
-46.245222	0.037759	0.950912
-46.397974	3.399325	0.955917
-46.461537	3.295665	0.960922
-46.627323	4.034920	0.965926
-47.560692	5.433064	0.970931
-47.431393	6.178700	0.975936
-47.721754	-1.838120	0.980941
-47.977957	2.310430	0.985946
-48.579628	-9.565936	0.990950
-49.284052	10.885892	0.995955
-49.173460	-0.933378	1.000960
-49.414064	5.789509	1.005965
-49.560520	-3.901359	1.010970
-49.376627	-7.257758	1.015974
-49.748921	1.172277	1.020979
-49.557160	-5.796318	1.025984
-50.628655	-1.862065	1.030989
-50.935785	2.114860	1.035994
-51.053723	-1.565356	1.040998
-51.388229	3.945412	1.046003
-50.933664	-0.140274	1.051008
-51.309738	3.156686	1.056013
-51.746620	-4.955485	1.061018
-52.564985	-0.396664	1.066022
-53.005019	3.621167	1.071027
-52.651020	-3.413209	1.076032
-52.579677	2.367879	1.081037
-52.726217	4.634357	1.086042
-53.316883	13.179213	1.091046
-53.970980	8.541388	1.096051
-54.205269	0.910899	1.101056
-54.196253	15.799480	1.106061
-54.207670	2.843565	1.111066
-53.996729	8.351203	1.116070
-55.131116	11.747344	1.121075
-55.272702	3.633819	1.126080
-55.674016	9.715881	1.131085
-56.064118	1.047367	1.136090
-55.976089	9.666116	1.141094
-55.984574	1.856940	1.146099
-56.080231	5.326961	1.151104
-56.880165	4.360638	1.156109
-57.248763	3.381433	1.161114
-57.216308	8.959904	1.166118
-57.692492	7.689990	1.171123
-57.445267	2.635861	1.176128
-57.244231	9.403356	1.181133
-57.983907	10.779061	1.186138
-58.660398	2.069681	1.191142
-58.921274	9.806521	1.196147
-59.055963	12.340464	1.201152
-59.277199	7.953993	1.206157
-59.375413	2.518341	1.211162
-59.423820	10.457723	1.216166
-60.439003	12.571997	1.221171
-60.638038	7.784484	1.226176
-60.922253	4.871546	1.231181
-61.053487	13.676190	1.236186
-60.870114	5.017669	1.241190
-61.062511	16.057245	1.246195
-61.037409	4.334081	1.251200
-61.186833	3.951513	1.256205
-61.885343	7.212282	1.261210
-62.436705	9.939981	1.266214
-62.425252	7.713045	1.271219
-62.088833	2.039135	1.276224
-62.989893	8.938357	1.281229
-63.501440	6.311200	1.286234
-63.864478	1.721462	1.291238
-64.024535	10.422054	1.296243
-63.828569	7.603289	1.301248
-63.997077	9.934366	1.306253
-64.240344	7.301740	1.311258
-64.162816	-0.131181	1.316262
-65.182083	6.296185	1.321267
-65.242983	5.045935	1.326272
-65.477135	2.025578	1.331277
-65.336120	4.172516	1.336282
-65.429210	-0.073240	1.341286
-66.192909	10.913362	1.346291
-66.506020	1.307549	1.351296
-66.624222	7.948649	1.356301
-66.912297	11.538568	1.361306
-66.865829	5.469921	1.366310
-68.127827	9.336714	1.371315
-68.287163	0.974364	1.376320
-68.506050	1.354616	1.381325
-68.678378	2.451485	1.386330
-68.446697	2.709329	1.391334
-68.693389	-1.115838	1.396339
-68.502845	5.230463	1.401344
-68.808151	3.618693	1.406349
-68.905137	20.297095	1.411354
-69.395811	6.841291	1.416358
-69.970660	21.544911	1.421363
-70.000968	5.899580	1.426368
-70.856539	7.529924	1.431373
-71.082969	13.273215	1.436378
-71.475898	-1.602568	1.441382
-71.661234	2.271952	1.446387
-71.192083	7.958390	1.451392
-71.639314	6.339691	1.456397
-71.883129	4.873334	1.461402
-71.892419	4.355832	1.466406
-72.607454	9.394693	1.471411
-72.818486	4.592295	1.476416
-73.438844	6.466407	1.481421
-73.748135	10.904598	1.486426
-73.412013	4.689033	1.491430
-73.708778	9.960449	1.496435
-73.623766	-4.024758	1.501440
-73.684570	6.726206	1.506445
-73.982354	-5.311167	1.511450
-74.405537	-5.012081	1.516454
-75.269424	2.860619	1.521459
-74.860869	4.163660	1.526464
-75.864885	2.917450	1.531469
-76.328119	-1.596535	1.536474
-76.055295	-6.495469	1.541478
-76.611732	6.546542	1.546483
-76.371070	-2.984853	1.551488
-76.702746	2.466255	1.556493
-76.904048	-4.927388	1.561498
-76.559961	-6.603567	1.566502
-77.147564	-1.936086	1.571507
-77.685463	-8.027915	1.576512
-78.166588	4.346789	1.581517
-78.209395	0.932359	1.586522
-78.072886	-4.489007	1.591526
-79.182011	4.969919	1.596531
-79.483808	3.501701	1.601536
-79.834134	-4.638483	1.606541
-79.934400	2.639315	1.611546
-79.563307	-0.343251	1.616550
-79.904249	5.737019	1.621555
-79.774228	-3.915782	1.626560
-80.388069	-0.694458	1.631565
-80.416822	0.798352	1.636570
-80.859361	7.124387	1.641574
-81.590436	6.807661	1.646579
-81.422220	2.548415	1.651584
-81.406850	9.081216	1.656589
-82.020793	-2.552210	1.661594
-82.676352	-2.570757	1.666598
-83.020017	8.922459	1.671603
-82.669520	6.461816	1.676608
-82.897001	-0.557553	1.681613
-82.978293	-0.617539	1.686618
-82.858715	4.271448	1.691622
-83.724660	3.504860	1.696627
-84.310797	-1.678790	1.701632
-84.297594	6.860081	1.706637
-84.627237	4.780772	1.711642
-84.620524	-0.811220	1.716646
-84.674996	-0.927234	1.721651
-85.052942	-2.348929	1.726656
-85.788970	9.020311	1.731661
-86.065678	4.702302	1.736666
-86.063501	5.663983	1.741670
-86.278534	10.144406	1.746675
-86.237704	0.148431	1.751680
-85.915940	7.663194	1.756685
-87.287392	4.728200	1.761690
-87.493100	5.946206	1.766694
-87.815631	8.437400	1.771699
-87.657045	7.576662	1.776704
-87.710985	2.822292	1.781709
-88.321408	12.090481	1.786714
-88.613971	2.087749	1.791718
-89.063693	8.145452	1.796723
-89.207458	0.822700	1.801728
-88.987662	4.987684	1.806733
-89.095348	8.818198	1.811738
-89.307024	0.550526	1.816742
-90.225215	4.868168	1.821747
-90.232703	1.942646	1.826752
-90.497116	6.165754	1.831757
-90.955270	9.670825	1.836762
-90.573448	2.537043	1.841766
-91.481186	8.279283	1.846771
-92.064950	7.528606	1.851776
-92.174123	3.712182	1.856781
-92.224541	4.486137	1.861786
-92.124099	8.644705	1.866790
-92.464938	9.174053	1.871795
-92.353678	-0.501890	1.876800
-92.381289	7.571079	1.881805
-92.960096	5.386057	1.886810
-93.376447	3.711449	1.891814
-94.011214	14.430605	1.896819
-93.811629	5.117606	1.901824
-94.735200	6.121893	1.906829
-95.243829	-2.059901	1.911834
-94.693217	3.108756	1.916838
-95.095841	7.800520	1.921843
-95.293595	-1.101028	1.926848
-95.046133	4.265513	1.931853
-95.471681	8.547611	1.936858
-95.716285	-3.493123	1.941862
-96.634210	3.989557	1.946867
-96.662187	0.477378	1.951872
-96.909667	-2.410946	1.956877
-97.274547	9.319583	1.961882
-96.976140	-4.038927	1.966886
-97.443702	13.106961	1.971891
-97.767936	1.912705	1.976896
-98.042657	6.437028	1.981901
-98.253828	9.242771	1.986906
-98.156080	-0.413872	1.991910
-98.697210	-3.106474	1.996915
-99.423893	4.936880	2.006912
-98.963673	5.868172	2.016909
-98.294027	9.391493	2.026906
-97.420904	7.887743	2.036902
-97.079490	2.013617	2.046899
-97.182717	0.599369	2.056896
-95.959030	-0.049350	2.066893
-95.769741	5.756481	2.076890
-95.538985	2.477893	2.086886
-94.967867	8.789590	2.096883
-94.276530	1.544706	2.106880
-93.697726	3.575372	2.116877
-93.247076	2.395210	2.126874
-92.783726	0.209105	2.136870
-92.086334	1.079321	2.146867
-91.340125	2.529996	2.156864
-91.429125	13.464560	2.166861
-90.984533	7.715622	2.176858
-89.867094	5.599464	2.186854
-89.866024	8.669746	2.196851
-89.591030	8.118995	2.206848
-88.798890	9.095150	2.216845
-88.365780	5.079069	2.226842
-87.598681	6.574101	2.236838
-87.259889	7.901219	2.246835
-86.673585	8.201713	2.256832
-86.173064	12.429082	2.266829
-85.538816	4.396928	2.276826
-85.221140	6.371478	2.286822
-84.993555	4.720111	2.296819
-83.900106	3.179605	2.306816
-83.457663	7.435389	2.316813
-83.496432	9.763261	2.326810
-82.821800	3.584646	2.336806
-82.364523	7.125533	2.346803
-82.018386	5.337470	2.356800
-81.276146	3.909880	2.366797
-80.732950	6.530070	2.376794
-79.775263	4.371319	2.386790
-79.475614	-2.157429	2.396787
-79.190790	0.020257	2.406784
-79.274255	2.880379	2.416781
-78.048615	2.028349	2.426778
-77.381722	-0.069748	2.436774
-77.195290	4.338090	2.446771
-77.009390	1.554095	2.456768
-75.980712	3.525081	2.466765
-75.875945	4.973803	2.476762
-75.081299	6.729803	2.486758
-74.561251	3.818425	2.496755
-74.421243	0.824008	2.506752
-73.606410	-4.319898	2.516749
-73.069597	3.530276	2.526746
-73.159355	4.401677	2.536742
-71.816540	7.811131	2.546739
-71.611736	9.348964	2.556736
-71.472090	10.105800	2.566733
-70.603020	7.274439	2.576730
-70.137977	11.575979	2.586726
-69.910524	7.596355	2.596723
-69.035896	13.953615	2.606720
-68.472064	14.482992	2.616717
-68.423548	8.058419	2.626714
-67.863621	9.708253	2.636710
-67.177778	6.795355	2.646707
-66.672989	7.843747	2.656704
-65.495136	10.100892	2.666701
-65.802146	11.534791	2.676698
-65.338915	18.601763	2.686694
-64.871507	9.104377	2.696691
-63.870713	8.641261	2.706688
-63.617720	3.093445	2.716685
-63.374154	6.389120	2.726682
-62.700249	8.792868	2.736678
-62.205948	5.273808	2.746675
-61.969639	8.050116	2.756672
-61.095504	6.257028	2.766669
-60.733009	8.549108	2.776666
-59.832996	7.872542	2.786662
-59.131627	7.403843	2.796659
-58.945086	8.157967	2.806656
-58.854985	2.724935	2.816653
-58.545027	7.190150	2.826650
-58.156967	10.751715	2.836646
-56.855121	9.860671	2.846643
-56.296922	7.786317	2.856640
-56.115282	10.852046	2.866637
-56.236458	7.156885	2.876634
-54.934651	8.587063	2.886630
-55.128046	1.997652	2.896627
-53.841639	6.934966	2.906624
-53.135500	10.475278	2.916621
-52.993682	5.404566	2.926618
-53.045977	6.136523	2.936614
-52.284795	5.000069	2.946611
-51.645662	2.558760	2.956608
-51.382694	6.882535	2.966605
-50.424130	5.886325	2.976602
-50.008576	4.938762	2.986598
-49.784750	4.894218	2.996595
-48.773191	9.695104	3.006592
-48.213662	8.207429	3.016589
-48.205393	6.771592	3.026586
-48.129809	5.422224	3.036582
-46.769705	-3.941213	3.046579
-46.630580	5.635020	3.056576
-46.422030	0.584446	3.066573
-45.254219	9.631369	3.076570
-45.041225	-0.551773	3.086566
-45.167918	4.100632	3.096563
-44.226393	-1.106784	3.106560
-43.744256	4.606550	3.116557
-42.475011	1.917779	3.126554
-42.724880	10.152229	3.136550
-42.097761	6.447048	3.146547
-41.941273	1.883317	3.156544
-40.803710	4.967240	3.166541
-40.675490	9.634170	3.176538
-40.392451	6.295279	3.186534
-39.529189	-1.255189	3.196531
-39.329614	5.063638	3.206528
-38.338908	3.473393	3.216525
-37.493882	3.728616	3.226522
-37.985973	7.416227	3.236518
-37.077805	5.129350	3.246515
-36.363557	5.449303	3.256512
-35.837922	7.694915	3.266509
-35.807502	8.220484	3.276506
-35.478326	0.912276	3.286502
-34.357210	4.340547	3.296499
-33.797907	3.265610	3.306496
-33.931799	1.850847	3.316493
-33.274834	1.938010	3.326490
-32.894191	2.744316	3.336486
-31.788440	0.034313	3.346483
-31.442289	5.423308	3.356480
-31.588789	3.587359	3.366477
-30.238383	4.316771	3.376474
-29.842138	12.216462	3.386470
-29.899733	4.966837	3.396467
-29.237676	-0.078377	3.406464
-28.668560	1.926485	3.416461
-28.022542	2.948775	3.426458
-27.118357	2.296367	3.436454
-27.001661	5.878431	3.446451
-26.758345	-2.527644	3.456448
-26.238488	-2.364579	3.466445
-25.148258	4.746895	3.476442
-25.186316	5.017175	3.486438
-24.854346	10.469216	3.496435
-23.980968	1.792572	3.506432
-23.600215	1.824134	3.516429
-23.025141	0.911306	3.526426
-22.132533	7.599377	3.536422
-21.739763	9.592638	3.546419
-21.870966	9.849467	3.556416
-21.511424	4.900474	3.566413
-20.502339	6.025701	3.576410
-20.173271	8.528572	3.586406
-19.237101	10.365602	3.596403
-18.829033	11.593611	3.606400
-18.570902	5.402285	3.616397
-18.464153	9.982036	3.626394
-17.515608	2.684524	3.636390
-17.226700	7.154456	3.646387
-16.410535	11.609611	3.656384
-15.887094	7.671604	3.666381
-15.564943	6.264598	3.676378
-15.011561	3.374533	3.686374
-14.142297	3.887025	3.696371
-14.101640	3.630940	3.706368
-13.830207	6.101206	3.716365
-13.062382	7.328832	3.726362
-12.490984	7.879634	3.736358
-12.124954	11.373477	3.746355
-11.135466	7.389222	3.756352
-10.500049	5.050025	3.766349
-10.752382	5.746092	3.776346
-10.725464	13.826344	3.786342
-9.626277	12.318832	3.796339
-9.255459	10.168419	3.806336
-8.174020	11.561139	3.816333
-7.873307	12.572881	3.826330
-7.891039	9.886298	3.836326
-7.010820	12.740571	3.846323
-6.431326	3.935430	3.856320
-6.160994	6.813048	3.866317
-5.295806	8.449138	3.876314
-4.860435	11.571275	3.886310
-4.685305	11.301413	3.896307
-4.019654	9.441634	3.906304
-3.504482	16.969036	3.916301
-3.305322	19.982337	3.926298
-2.673514	33.398868	3.936294
-2.347106	35.503560	3.946291
-1.866828	45.815165	3.956288
-1.553260	65.936829	3.966285
-1.263616	77.653986	3.976282
-0.819078	103.232633	3.986278
0.000000	120.454056	3.991283
-0.272092	125.551848	3.996288
0.362907	128.327284	4.001293
0.260189	146.603593	4.006298
0.494934	148.437426	4.011302
0.692767	154.729812	4.016307
0.521282	167.869153	4.021312
0.668956	160.969029	4.026317
0.614344	162.942628	4.031322
0.875014	159.062477	4.036326
0.780576	171.187552	4.041331
0.732827	165.318694	4.046336
1.014367	162.745022	4.051341
0.793505	154.794170	4.056346
0.771615	159.295697	4.061350
0.861769	157.389972	4.066355
0.552004	169.374928	4.071360
1.057950	159.259852	4.076365
0.669971	166.034196	4.081370
0.500592	165.434132	4.086374
0.997661	170.365566	4.091379
0.620967	171.550675	4.096384
0.906497	158.136431	4.101389
0.754235	167.723713	4.106394
0.486107	165.533781	4.111398
0.994885	182.134856	4.116403
1.105596	190.322200	4.121408
1.018347	190.275429	4.126413
0.805657	197.434773	4.131418
1.221035	191.236717	4.136422
1.098715	194.139289	4.141427
0.923449	197.662268	4.146432
0.883578	195.522116	4.151437
1.190104	192.812705	4.156442
0.911245	198.569368	4.161446
1.275609	195.181128	4.166451
1.195412	200.754020	4.171456
1.143627	198.442107	4.176461
0.749758	197.518657	4.181466
1.252100	197.978908	4.186470
1.305269	195.527812	4.191475
0.965057	204.733014	4.196480
1.144667	190.364895	4.201485
0.869276	202.057013	4.206490
0.963545	203.186787	4.211494
1.010171	195.944344	4.216499
0.806965	196.726589	4.221504
1.328668	191.827898	4.226509
1.612108	203.319344	4.231514
1.604665	199.037671	4.236518
1.345901	198.323041	4.241523
0.914581	205.550088	4.246528
1.181513	190.264753	4.251533
1.167175	198.669878	4.256538
1.242394	191.581052	4.261542
1.182691	191.676527	4.266547
1.107378	198.800837	4.271552
1.449589	210.754440	4.276557
1.557899	219.383774	4.281562
1.328639	212.007265	4.286566
1.138561	208.560791	4.291571
1.134694	235.305640	4.296576
1.491874	222.981864	4.301581
1.595663	234.624762	4.306586
1.934414	229.764678	4.311590
1.691788	216.745959	4.316595
1.318065	202.558453	4.321600
1.211588	198.078968	4.326605
1.568114	216.795726	4.331610
1.697683	225.181326	4.336614
1.756566	224.302722	4.341619
1.683245	218.498939	4.346624
1.601369	204.237651	4.351629
1.480834	196.442744	4.356634
1.288739	202.765552	4.361638
1.664607	206.563956	4.366643
1.327213	224.924520	4.371648
1.948066	221.329727	4.376653
1.964589	232.525144	4.381658
1.471007	216.124784	4.386662
1.531817	192.186695	4.391667
1.412032	219.378734	4.396672
1.754415	218.607477	4.401677
1.464091	234.381152	4.406682
1.735191	229.086132	4.411686
1.694627	228.953808	4.416691
1.577365	233.462930	4.421696
1.899106	231.998780	4.426701
1.940334	232.295405	4.431706
1.638245	230.730132	4.436710
2.034935	230.792804	4.441715
1.997773	238.293410	4.446720
2.016555	239.992568	4.451725
1.890419	223.420589	4.456730
1.708196	223.097200	4.461734
1.389212	218.679069	4.466739
1.598474	224.919478	4.471744
2.086768	221.413578	4.476749
1.576239	238.680971	4.481754
1.587394	236.911017	4.486758
2.020865	233.033071	4.491763
1.819743	237.048573	4.496768
2.024308	239.857179	4.501773
1.778259	240.974632	4.506778
1.897285	239.439506	4.511782
2.181224	233.554382	4.516787
1.645178	238.333966	4.521792
1.652689	236.651431	4.526797
1.915916	245.842469	4.531802
1.628931	243.449946	4.536806
1.868804	238.794926	4.541811
2.043147	262.139149	4.546816
2.162909	263.646312	4.551821
2.151035	262.562457	4.556826
2.193773	261.850286	4.561830
2.161277	245.658118	4.566835
1.760178	253.766308	4.571840
1.990976	254.870072	4.576845
2.125125	259.833492	4.581850
2.230432	259.585511	4.586854
2.380818	257.848680	4.591859
2.133678	272.447680	4.596864
2.132691	264.778597	4.601869
2.176324	272.940075	4.606874
2.303340	274.965359	4.611878
2.310520	266.749266	4.616883
2.170167	269.160671	4.621888
2.331078	262.028252	4.626893
2.313376	273.929705	4.631898
2.234378	267.775038	4.636902
2.492790	261.245566	4.641907
2.220385	271.606095	4.646912
2.257862	264.800791	4.651917
2.266298	275.460894	4.656922
2.355802	271.983692	4.661926
2.186810	265.359898	4.666931
1.976112	261.825761	4.671936
2.338064	264.972793	4.676941
2.432794	271.799710	4.681946
2.479899	270.225758	4.686950
2.287190	262.452808	4.691955
2.226487	264.063291	4.696960
2.719378	268.619179	4.701965
2.527139	264.609336	4.706970
2.310481	268.826400	4.711974
2.267447	259.969461	4.716979
2.203305	272.544802	4.721984
2.586851	263.114523	4.726989
2.306077	275.924950	4.731994
2.211133	266.118154	4.736998
2.460072	272.023604	4.742003
2.336094	274.879407	4.747008
2.104730	260.779506	4.752013
2.422521	281.924717	4.757018
2.700086	284.099644	4.762022
3.068622	291.018353	4.767027
2.555815	294.150918	4.772032
2.765549	283.055051	4.777037
2.371956	268.598677	4.782042
2.273409	278.637278	4.787046
2.891364	289.029839	4.792051
2.818264	291.841229	4.797056
2.934489	285.281773	4.802061
2.487120	278.776586	4.807066
2.757388	290.728132	4.812070
3.015246	292.393409	4.817075
2.511693	279.585864	4.822080
2.292217	283.278752	4.827085
2.806625	291.358594	4.832090
2.454896	298.188566	4.837094
2.305809	308.078874	4.842099
2.547279	300.046611	4.847104
2.579646	297.145125	4.852109
2.749301	293.707157	4.857114
2.693976	302.833472	4.862118
3.049602	287.115481	4.867123
2.819630	308.947521	4.872128
2.765708	293.249553	4.877133
3.016615	296.174915	4.882138
3.012778	301.455341	4.887142
2.959128	297.494703	4.892147
2.433287	299.915162	4.897152
2.706711	298.134022	4.902157
2.654752	310.152841	4.907162
2.747719	316.454336	4.912166
3.213241	321.881843	4.917171
2.983373	325.333963	4.922176
3.018786	332.843734	4.927181
3.521399	328.428310	4.932186
3.140851	323.296193	4.937190
3.262734	294.097923	4.942195
2.964832	296.734158	4.947200
2.933830	297.138810	4.952205
3.111998	301.262815	4.957210
3.031381	291.166057	4.962214
3.209171	297.141974	4.967219
3.001219	289.445323	4.972224
3.126886	305.024245	4.977229
3.128463	310.733619	4.982234
3.067734	309.505708	4.987238
3.014221	309.491344	4.992243
3.036436	321.333852	4.997248
3.092089	323.431806	5.002253
3.519092	326.803393	5.007258
3.445277	325.901331	5.012262
3.342010	313.678732	5.017267
3.048455	308.770200	5.022272
3.064226	309.915717	5.027277
3.078647	327.172817	5.032282
3.396303	322.952121	5.037286
3.697566	330.782489	5.042291
3.449317	323.400975	5.047296
3.220206	310.360014	5.052301
3.101801	312.762077	5.057306
3.154395	308.307276	5.062310
3.234340	320.592182	5.067315
3.209315	319.614183	5.072320
3.056009	320.230339	5.077325
3.074102	326.171197	5.082330
3.283141	323.481524	5.087334
3.700451	318.841749	5.092339
3.459041	320.919045	5.097344
3.501399	325.897853	5.102349
3.420967	323.514098	5.107354
3.185067	319.800910	5.112358
3.242185	326.072522	5.117363
3.137942	327.796360	5.122368
3.479554	309.976249	5.127373
3.450567	328.746394	5.132378
3.574857	318.279539	5.137382
3.701476	319.629601	5.142387
3.353566	326.424623	5.147392
3.747558	321.629471	5.152397
3.356821	322.344156	5.157402
3.400298	321.472335	5.162406
3.706628	341.445922	5.167411
3.465098	350.098317	5.172416
3.742549	350.849775	5.177421
3.784280	342.712973	5.182426
3.765571	338.877959	5.187430
3.482814	334.870329	5.192435
3.333202	342.996694	5.197440
3.720406	347.846601	5.202445
3.769770	341.252197	5.207450
3.821761	364.564508	5.212454
3.985608	357.460071	5.217459
3.548427	345.105281	5.222464
3.530343	359.185566	5.227469
3.731274	366.224940	5.232474
3.937802	362.865115	5.237478
4.089998	360.307951	5.242483
3.897484	355.432527	5.247488
3.581768	339.663236	5.252493
3.780776	346.099149	5.257498
3.700136	355.537878	5.262502
4.276979	352.464223	5.267507
3.893944	365.803743	5.272512
3.819641	350.935324	5.277517
4.004268	353.586635	5.282522
3.826513	357.039326	5.287526
3.779225	352.389600	5.292531
3.535409	360.348832	5.297536
3.790091	355.319300	5.302541
4.236480	359.690029	5.307546
3.735204	364.206218	5.312550
3.908135	362.840344	5.317555
3.736242	361.887303	5.322560
4.137165	358.102016	5.327565
4.011340	359.917227	5.332570
3.836057	365.379811	5.337574
3.953526	359.173896	5.342579
3.923563	359.603042	5.347584
4.213512	347.172976	5.352589
4.178764	356.770455	5.357594
3.952862	347.817899	5.362598
4.227174	356.522479	5.367603
3.834783	346.954796	5.372608
3.992922	356.811235	5.377613
4.365518	347.992601	5.382618
3.910658	349.955119	5.387622
4.080930	341.748537	5.392627
4.098683	358.433809	5.397632
4.078185	351.874425	5.402637
4.068107	355.422034	5.407642
4.248078	361.930454	5.412646
4.065243	357.416384	5.417651
4.126982	366.277049	5.422656
4.246635	366.672789	5.427661
3.970711	378.844297	5.432666
3.961482	372.794275	5.437670
4.091028	365.233303	5.442675
3.563884	370.262534	5.447680
4.100740	373.428434	5.452685
4.169613	371.481805	5.457690
4.141619	378.837520	5.462694
4.540477	375.943625	5.467699
3.994062	380.118926	5.472704
4.066465	380.815974	5.477709
4.505162	391.726376	5.482714
4.069996	411.802465	5.487718
4.722294	399.582202	5.492723
4.908099	404.605994	5.497728
4.787724	398.802026	5.502733
4.919773	386.490858	5.507738
4.436262	384.867647	5.512742
4.667222	382.534434	5.517747
4.327525	389.351014	5.522752
4.528052	377.821727	5.527757
4.468417	381.967984	5.532762
4.464311	386.697789	5.537766
4.388477	380.223207	5.542771
4.073801	386.852053	5.547776
4.196059	383.299959	5.552781
4.854178	388.155326	5.557786
4.550456	404.721126	5.562790
4.685128	404.739099	5.567795
4.496776	408.263105	5.572800
5.013191	406.278916	5.577805
4.717836	390.665339	5.582810
4.558899	386.066216	5.587814
5.009603	379.746228	5.592819
4.311089	389.312242	5.597824
4.441474	394.546743	5.602829
4.811498	398.578692	5.607834
4.466011	415.445597	5.612838
4.981887	402.450146	5.617843
4.625988	404.402631	5.622848
4.793581	414.961058	5.627853
4.799121	408.592686	5.632858
4.887194	421.351158	5.637862
5.191770	402.746828	5.642867
4.615413	402.414872	5.647872
4.502511	390.724176	5.652877
4.799122	407.842589	5.657882
4.704026	414.568839	5.662886
4.802648	412.303168	5.667891
4.625345	419.226011	5.672896
4.492074	409.626419	5.677901
4.689169	418.002248	5.682906
4.599157	421.820969	5.687910
4.887032	411.576517	5.692915
4.770847	415.088894	5.697920
4.524355	409.519254	5.702925
4.808763	422.429374	5.707930
4.628209	410.302044	5.712934
5.275288	432.527686	5.717939
5.189277	436.356897	5.722944
5.142712	418.462592	5.727949
5.113604	414.398226	5.732954
4.784695	416.695691	5.737958
4.977608	414.467120	5.742963
4.810383	416.669498	5.747968
4.922424	442.345462	5.752973
5.568621	436.177533	5.757978
4.748628	441.183459	5.762982
5.355983	438.240989	5.767987
5.365581	440.747507	5.772992
5.086760	427.894807	5.777997
4.835435	423.572476	5.783002
4.661608	430.342919	5.788006
5.281136	431.333622	5.793011
5.214327	444.751868	5.798016
5.449423	439.989351	5.803021
5.270969	434.589788	5.808026
5.075302	439.604318	5.813030
5.423021	429.479993	5.818035
5.680523	441.600889	5.823040
4.990198	424.689224	5.828045
5.412074	427.524698	5.833050
5.476805	444.961260	5.838054
5.187438	424.109315	5.843059
5.015726	428.634299	5.848064
4.970784	426.183201	5.853069
5.433970	439.636587	5.858074
5.512875	432.080892	5.863078
5.450206	439.544376	5.868083
5.367987	444.981743	5.873088
5.456817	436.453928	5.878093
5.358478	434.026057	5.883098
4.999717	448.944668	5.888102
5.160688	440.126720	5.893107
5.126788	443.642869	5.898112
5.246487	446.207553	5.903117
5.473969	437.318533	5.908122
5.401880	444.348702	5.913126
5.386680	430.401947	5.918131
4.999776	445.762349	5.923136
5.335701	439.121731	5.928141
5.409478	444.450843	5.933146
5.027153	454.152880	5.938150
5.566401	465.209895	5.943155
5.706454	468.905369	5.948160
5.736979	472.952105	5.953165
5.942682	477.240802	5.958170
5.698077	476.162047	5.963174
5.592740	454.286380	5.968179
5.349789	457.095778	5.973184
5.457463	459.977559	5.978189
5.932024	469.304877	5.983194
5.428152	476.468666	5.988198
5.956656	470.238880	5.993203
5.911367	470.550695	5.998208
5.737944	461.362886	6.003213
5.813847	448.446517	6.008218
5.580854	448.954796	6.013222
5.877439	448.533926	6.018227
5.707511	448.755843	6.023232
5.638776	450.705669	6.028237
5.763432	440.966356	6.033242
5.424510	440.529654	6.038246
5.486727	433.643432	6.043251
5.640411	446.735589	6.048256
5.617068	447.683265	6.053261
5.570710	451.853787	6.058266
5.535312	465.631197	6.063270
5.942847	469.097882	6.068275
5.750882	451.559841	6.073280
5.409065	443.362062	6.078285
5.628167	452.283391	6.083290
5.772673	465.855563	6.088294
5.653447	466.942602	6.093299
5.268575	465.796362	6.098304
5.859987	470.708062	6.103309
5.769908	473.987256	6.108314
5.635871	473.857551	6.113318
5.715616	477.496795	6.118323
5.863840	471.689256	6.123328
5.389039	455.585448	6.128333
5.558336	456.531083	6.133338
5.777464	475.963330	6.138342
5.907882	466.763585	6.143347
5.822412	458.263477	6.148352
5.448606	446.425349	6.153357
5.647380	458.334087	6.158362
5.509540	469.082130	6.163366
5.611485	460.184641	6.168371
6.112772	474.732762	6.173376
5.986888	465.126883	6.178381
5.807482	447.741956	6.183386
5.362042	455.246110	6.188390
5.612035	447.734154	6.193395
5.606982	444.946259	6.198400
5.512405	446.089699	6.203405
5.540974	441.272127	6.208410
5.248316	458.014822	6.213414
5.838712	463.825838	6.218419
5.825189	476.429287	6.223424
5.867674	468.750255	6.228429
5.687336	451.177736	6.233434
5.444488	457.667674	6.238438
5.697434	461.984273	6.243443
5.791992	478.027558	6.248448
5.626984	467.278207	6.253453
6.124801	465.346906	6.258458
5.336197	455.398016	6.263462
5.451944	455.639119	6.268467
5.613742	472.102215	6.273472
5.839736	469.943247	6.278477
5.878063	474.957003	6.283482
5.753060	455.384850	6.288486
5.645133	447.983145	6.293491
5.571686	448.440691	6.298496
5.425574	449.982437	6.303501
5.757443	446.930799	6.308506
5.566525	467.447643	6.313510
6.122515	462.092837	6.318515
5.669941	458.346855	6.323520
5.323044	452.091953	6.328525
5.836042	451.452708	6.333530
5.696836	459.475207	6.338534
5.626076	443.712979	6.343539
5.740665	455.938402	6.348544
5.550130	455.095280	6.353549
5.626866	449.547485	6.358554
5.773682	458.021620	6.363558
5.893363	451.342246	6.368563
6.031308	448.641807	6.373568
5.766167	454.381499	6.378573
6.120431	447.448982	6.383578
5.783921	452.949487	6.388582
6.018183	442.419091	6.393587
5.790674	449.642661	6.398592
5.895746	451.673371	6.403597
5.688010	443.963090	6.408602
5.658381	447.402175	6.413606
5.925621	440.933420	6.418611
5.926953	442.537222	6.423616
5.882560	448.526140	6.428621
5.524051	423.419248	6.433626
5.319792	430.583621	6.438630
5.762241	437.733369	6.443635
5.967157	447.689572	6.448640
5.686503	436.333185	6.453645
5.630493	426.994486	6.458650
5.516453	435.888975	6.463654
5.746904	429.853286	6.468659
6.102819	432.249496	6.473664
5.537907	425.760514	6.478669
5.645091	418.195516	6.483674
4.990625	420.160248	6.488678
5.686181	433.514752	6.493683
5.532119	438.471598	6.498688
5.613626	437.522354	6.503693
5.907925	436.090246	6.508698
5.638976	449.198184	6.513702
5.790838	447.787837	6.518707
5.589648	443.906890	6.523712
5.642246	451.594715	6.528717
5.501578	446.806292	6.533722
5.433379	455.936799	6.538726
5.693934	444.569894	6.543731
5.543637	446.378209	6.548736
5.836617	444.065715	6.553741
5.697364	443.526859	6.558746
5.359730	446.255910	6.563750
5.468797	437.756221	6.568755
5.537596	439.117920	6.573760
5.670135	447.485689	6.578765
5.770020	442.667676	6.583770
5.874511	442.701588	6.588774
5.671941	431.320364	6.593779
5.477230	439.681634	6.598784
5.445474	440.270802	6.603789
5.768269	434.343763	6.608794
5.425013	443.032061	6.613798
5.760511	438.637711	6.618803
5.721737	444.104006	6.623808
5.996410	442.357962	6.628813
6.127829	436.437292	6.633818
5.593253	444.404562	6.638822
5.968130	443.964342	6.643827
5.976923	448.970836	6.648832
5.493227	440.270472	6.653837
5.987336	436.601964	6.658842
5.454299	443.518591	6.663846
5.897838	437.829089	6.668851
5.592420	436.500428	6.673856
5.522996	434.059590	6.678861
6.024357	435.707926	6.683866
5.567873	434.050351	6.688870
5.465430	424.732941	6.693875
5.430931	433.632733	6.698880
5.722605	446.406908	6.703885
5.503215	433.337500	6.708890
5.155271	439.859498	6.713894
5.463438	447.783988	6.718899
5.371827	438.359020	6.723904
5.415638	447.531685	6.728909
5.621909	443.604909	6.733914
5.488088	446.984950	6.738918
5.601879	445.713489	6.743923
5.708654	447.081048	6.748928
5.357655	448.959625	6.753933
5.642050	443.670819	6.758938
5.356997	450.809189	6.763942
5.572336	460.317359	6.768947
5.941253	454.840158	6.773952
5.583370	453.401877	6.778957
5.641921	438.963261	6.783962
5.689385	470.094070	6.788966
5.595821	448.922251	6.793971
5.930346	458.150765	6.798976
5.927061	454.602630	6.803981
5.782027	450.994457	6.808986
5.590079	455.808895	6.813990
5.624701	450.131619	6.818995
5.804141	455.530879	6.824000
5.411229	447.704201	6.829005
5.586778	447.169358	6.834010
5.684731	443.042157	6.839014
5.526305	441.821699	6.844019
5.997699	442.519901	6.849024
5.576958	438.496472	6.854029
5.463605	446.987451	6.859034
5.453306	445.436187	6.864038
5.620183	451.646501	6.869043
5.739496	462.149207	6.874048
5.692546	467.535865	6.879053
6.101257	461.548743	6.884058
5.523127	472.528780	6.889062
5.540672	452.765259	6.894067
5.447402	441.378692	6.899072
5.375901	456.150000	6.904077
5.822139	458.838896	6.909082
5.580892	475.049448	6.914086
6.033227	476.812538	6.919091
5.546922	472.385382	6.924096
5.543432	480.655979	6.929101
6.095766	468.053413	6.934106
5.768594	464.518351	6.939110
5.309645	457.645535	6.944115
5.651757	460.812066	6.949120
5.672651	462.508926	6.954125
5.801839	467.640949	6.959130
5.539240	460.258682	6.964134
5.965995	456.022190	6.969139
6.050062	455.030889	6.974144
5.700984	455.596138	6.979149
5.826954	443.865729	6.984154
5.443099	458.121878	6.989158
5.743290	453.515625	6.994163
5.738701	458.016354	6.999168
5.737722	445.540464	7.004173
5.756827	445.791520	7.009178
5.505418	445.110685	7.014182
5.662264	446.060547	7.019187
5.591985	447.471276	7.024192
5.479834	441.675009	7.029197
5.720869	445.497432	7.034202
5.906310	447.877914	7.039206
5.755551	450.386269	7.044211
5.803314	445.898980	7.049216
5.434346	442.074468	7.054221
5.513533	437.927284	7.059226
5.465315	453.867266	7.064230
5.845187	441.701658	7.069235
5.851155	435.003792	7.074240
5.601506	444.125407	7.079245
5.877850	433.452213	7.084250
5.915081	448.757820	7.089254
5.598834	437.622088	7.094259
5.637051	442.163291	7.099264
5.537975	445.008203	7.104269
5.757633	442.539224	7.109274
5.407953	452.968286	7.114278
5.494531	449.132025	7.119283
5.554212	448.964487	7.124288
5.382549	455.972443	7.129293
5.892322	448.711945	7.134298
5.501689	445.743794	7.139302
5.864372	447.794282	7.144307
6.026060	446.203251	7.149312
5.543366	451.648496	7.154317
5.928957	450.640022	7.159322
5.953108	456.991719	7.164326
6.078166	439.929703	7.169331
5.972964	454.933191	7.174336
5.513393	454.115488	7.179341
5.417077	441.269711	7.184346
5.176146	457.003191	7.189350
5.473872	437.270341	7.194355
5.769825	445.158865	7.199360
5.894920	443.705094	7.204365
5.610709	446.369872	7.209370
5.548600	444.353227	7.214374
5.486794	440.600091	7.219379
5.869470	440.811388	7.224384
5.478581	451.018674	7.229389
5.693488	435.926278	7.234394
5.427431	450.727758	7.239398
5.649745	451.265963	7.244403
5.281992	444.962914	7.249408
5.939197	452.808022	7.254413
5.807917	444.663944	7.259418
5.616383	446.293897	7.264422
5.833381	449.773222	7.269427
5.784786	441.027098	7.274432
5.772732	448.528394	7.279437
5.670632	440.289917	7.284442
5.499995	452.456811	7.289446
5.519924	446.663872	7.294451
5.472547	437.352646	7.299456
5.589879	453.413846	7.304461
5.799578	443.655939	7.309466
5.615638	450.722747	7.314470
5.251999	450.652887	7.319475
5.875081	446.902489	7.324480
5.328179	447.652358	7.329485
5.627695	455.258341	7.334490
6.024485	476.922818	7.339494
5.812817	456.948163	7.344499
5.801768	458.131469	7.349504
5.558383	452.645059	7.354509
5.542073	443.576815	7.359514
5.777645	451.840545	7.364518
5.427783	450.398176	7.369523
5.813487	453.053765	7.374528
5.748138	456.586262	7.379533
5.605983	452.132527	7.384538
5.614966	451.416750	7.389542
5.521625	453.883160	7.394547
5.729126	461.521221	7.399552
5.589729	465.356006	7.404557
5.788753	463.140723	7.409562
5.436809	469.327274	7.414566
5.820306	466.055680	7.419571
5.919253	464.579591	7.424576
5.556715	458.364663	7.429581
5.551982	453.494679	7.434586
5.579334	461.390603	7.439590
5.842046	468.493609	7.444595
5.572133	455.249525	7.449600
5.432373	471.143683	7.454605
5.874567	475.484260	7.459610
5.730372	466.449567	7.464614
5.886819	466.403564	7.469619
5.766376	454.308490	7.474624
5.511990	452.705122	7.479629
5.788155	435.588739	7.484634
5.852207	444.145109	7.489638
5.665668	450.993330	7.494643
6.005478	444.222632	7.499648
5.583725	444.928734	7.504653
6.021331	432.883127	7.509658
5.536149	445.615204	7.514662
5.858740	446.711409	7.519667
5.677484	450.351849	7.524672
5.644843	458.034822	7.529677
6.004506	449.316726	7.534682
5.647194	455.324407	7.539686
5.585968	453.568757	7.544691
5.894549	452.234916	7.549696
5.771656	446.410135	7.554701
6.101362	444.399083	7.559706
5.849596	441.382531	7.564710
6.119715	440.140878	7.569715
5.775615	429.647367	7.574720
5.435161	422.581745	7.579725
5.680347	417.238064	7.584730
5.720271	437.094696	7.589734
5.883600	429.500486	7.594739
5.766264	417.492041	7.599744
5.604218	421.437303	7.604749
5.685987	417.854107	7.609754
5.509390	423.387369	7.614758
5.505290	413.081462	7.619763
5.522474	419.439326	7.624768
5.704388	436.754898	7.629773
5.891957	446.779573	7.634778
5.566643	432.437942	7.639782
5.683098	443.755118	7.644787
5.630926	435.315323	7.649792
5.381350	443.046766	7.654797
5.692282	443.906249	7.659802
5.938649	451.478295	7.664806
5.674306	444.819668	7.669811
6.085669	444.085442	7.674816
5.569294	435.984981	7.679821
5.638694	420.452470	7.684826
5.764736	423.318087	7.689830
5.710020	420.330536	7.694835
5.911696	422.728457	7.699840
5.363251	421.020869	7.704845
5.708619	408.386948	7.709850
5.827623	417.119694	7.714854
5.700310	419.589246	7.719859
5.734143	421.502091	7.724864
5.453436	425.252091	7.729869
5.604050	427.011367	7.734874
5.417713	426.841964	7.739878
5.589203	427.341607	7.744883
5.796070	422.513123	7.749888
5.508540	431.805351	7.754893
5.865355	429.959114	7.759898
5.843662	435.120204	7.764902
5.674323	421.343953	7.769907
5.554273	424.317423	7.774912
5.443884	427.359145	7.779917
5.816613	426.976500	7.784922
5.538943	437.633978	7.789926
5.479412	422.440838	7.794931
5.501011	433.619285	7.799936
5.673418	454.787972	7.804941
6.052945	448.900682	7.809946
5.578058	451.468423	7.814950
5.631803	442.393633	7.819955
5.951863	444.447515	7.824960
5.649752	431.394738	7.829965
5.909361	427.856143	7.834970
5.757919	429.160613	7.839974
5.376734	418.911196	7.844979
5.672229	425.895804	7.849984
5.549016	433.982042	7.854989
5.597576	421.893003	7.859994
5.546698	431.312851	7.864998
5.772601	449.111980	7.870003
5.887582	445.400364	7.875008
5.241335	441.623153	7.880013
5.744283	443.105684	7.885018
5.777222	444.453973	7.890022
5.797784	448.251369	7.895027
5.641963	438.609906	7.900032
5.449854	430.879686	7.905037
5.559741	450.230014	7.910042
5.557830	450.354219	7.915046
5.654618	451.188812	7.920051
6.010103	451.359221	7.925056
5.842482	457.357062	7.930061
5.701839	432.390648	7.935066
5.440776	437.385697	7.940070
5.134561	446.218227	7.945075
6.055185	454.235466	7.950080
5.912972	454.664223	7.955085
5.586192	445.421954	7.960090
5.491699	442.282136	7.965094
5.788216	444.201297	7.970099
5.749821	458.684684	7.975104
5.838771	443.902256	7.980109
5.603606	423.404211	7.985114
5.515019	434.972405	7.990118
5.597446	440.137526	7.995136
5.843229	441.884103	8.000154
5.297493	444.253306	8.005171
5.544511	446.677979	8.010189
5.758220	454.610824	8.015206
5.472319	454.229890	8.020224
5.814466	468.769047	8.025242
5.577291	459.611644	8.030259
5.639238	457.055370	8.035277
6.150699	458.358817	8.040294
6.146258	461.366862	8.045312
6.044457	439.377029	8.050330
5.392521	436.840917	8.055347
5.808785	423.583493	8.060365
5.710102	427.482704	8.065382
5.521260	423.536494	8.070400
5.683839	432.407400	8.075418
5.650412	450.953725	8.080435
5.648629	449.933446	8.085453
5.534566	450.668852	8.090470
5.785645	454.275674	8.095488
5.717606	450.328091	8.100506
5.773047	453.165446	8.105523
6.116905	452.994548	8.110541
5.941480	454.229655	8.115558
5.297850	454.414915	8.120576
5.903559	451.308545	8.125594
5.583193	445.113681	8.130611
6.055635	443.037487	8.135629
5.778967	447.161153	8.140646
5.516643	448.685661	8.145664
5.681890	454.153813	8.150682
5.830589	447.385279	8.155699
5.916486	451.908480	8.160717
5.908772	450.626737	8.165734
5.805281	444.272930	8.170752
5.692705	446.581966	8.175770
5.772357	451.956609	8.180787
5.638799	445.878972	8.185805
5.879555	460.343163	8.190822
5.725433	448.751690	8.195840
5.770015	439.343451	8.200858
5.602390	455.864168	8.205875
5.697423	448.777701	8.210893
6.126211	447.156460	8.215910
5.836215	448.834229	8.220928
5.784361	449.381439	8.225946
5.752278	455.686361	8.230963
5.958673	451.423405	8.235981
5.786385	467.993026	8.240998
6.135812	461.617405	8.246016
6.142689	460.869750	8.251034
5.710853	456.158149	8.256051
5.810991	459.510645	8.261069
5.830887	461.677148	8.266086
5.898411	474.904796	8.271104
5.978184	476.907601	8.276122
5.980132	490.961478	8.281139
6.293200	487.380245	8.286157
6.096890	463.179694	8.291174
5.870240	456.888155	8.296192
5.562193	449.885322	8.301210
6.032147	467.522082	8.306227
6.044151	477.818290	8.311245
6.477480	473.464294	8.316262
5.952254	464.526207	8.321280
5.939738	452.343734	8.326298
5.956469	459.624338	8.331315
5.717051	458.329321	8.336333
6.219183	470.580808	8.341350
6.040366	481.098670	8.346368
6.287510	475.999818	8.351386
6.034247	460.925361	8.356403
6.083473	451.814020	8.361421
6.000396	459.171735	8.366438
5.860688	456.671910	8.371456
5.987961	466.743298	8.376474
5.930386	486.799440	8.381491
6.146480	476.131894	8.386509
6.104577	482.966193	8.391526
5.986271	488.217492	8.396544
6.189043	479.878033	8.401562
6.313020	483.144329	8.406579
6.021776	474.277290	8.411597
6.322331	483.914825	8.416614
5.743775	474.467642	8.421632
6.184592	481.087255	8.426650
6.363720	487.207810	8.431667
6.337442	478.020859	8.436685
6.415352	461.482227	8.441702
6.052141	468.863213	8.446720
5.807064	448.719297	8.451738
6.040053	461.240600	8.456755
6.077594	471.109937	8.461773
6.295212	474.394804	8.466790
6.335374	483.482582	8.471808
6.043301	458.650952	8.476826
5.986371	465.295346	8.481843
5.798650	473.999705	8.486861
6.224751	471.347628	8.491878
6.247973	491.752454	8.496896
6.120424	479.120466	8.501914
6.049328	486.181295	8.506931
6.153786	482.033089	8.511949
6.504689	482.670108	8.516966
6.170517	484.635634	8.521984
6.260926	486.149088	8.527002
6.330127	483.761850	8.532019
5.927601	485.979763	8.537037
6.292344	490.836933	8.542054
6.004106	478.689868	8.547072
6.194907	481.472681	8.552090
6.255106	482.840174	8.557107
5.780696	482.366993	8.562125
6.619318	478.085753	8.567143
6.054723	490.531645	8.572160
6.299042	484.291568	8.577178
6.519481	487.449128	8.582195
6.315418	481.692315	8.587213
6.561082	486.809073	8.592231
6.271329	491.305110	8.597248
6.323856	490.267292	8.602266
6.318009	488.071158	8.607283
6.072838	484.968612	8.612301
6.154895	476.815013	8.617319
6.430055	491.130468	8.622336
6.640261	486.515470	8.627354
6.537967	490.781949	8.632371
6.140388	489.011793	8.637389
6.401995	481.770153	8.642407
6.435381	492.512841	8.647424
6.471490	489.564851	8.652442
6.266585	484.446330	8.657459
6.254890	489.833916	8.662477
6.786771	488.901096	8.667495
6.220371	494.195745	8.672512
6.545949	486.966065	8.677530
6.218920	497.559700	8.682547
6.185905	488.696426	8.687565
6.485705	478.752094	8.692583
5.997141	487.287030	8.697600
5.936558	490.537576	8.702618
6.418682	487.505155	8.707635
6.296296	475.659650	8.712653
6.307347	484.211606	8.717671
6.230834	501.711791	8.722688
6.606971	500.786109	8.727706
6.694887	506.395674	8.732723
6.134674	497.852539	8.737741
6.458212	501.047974	8.742759
6.135362	513.920471	8.747776
6.705879	510.250930	8.752794
7.012260	509.786976	8.757811
6.393879	502.959786	8.762829
6.494423	487.204328	8.767847
6.582211	490.457023	8.772864
6.527472	499.202006	8.777882
6.310180	488.297080	8.782899
6.367397	507.894707	8.787917
6.707599	506.250902	8.792935
6.491447	510.837025	8.797952
6.384019	500.563208	8.802970
6.620837	506.326771	8.807987
6.335770	510.101718	8.813005
6.501371	507.381683	8.818023
6.527798	512.088020	8.823040
6.739599	513.346328	8.828058
6.731337	513.852584	8.833075
6.934400	508.900150	8.838093
6.637371	502.417902	8.843111
6.457095	503.348859	8.848128
6.406196	504.043225	8.853146
6.722962	505.063563	8.858163
6.476275	504.257535	8.863181
6.619103	508.938042	8.868199
6.554194	502.479037	8.873216
6.415801	516.480161	8.878234
6.728862	510.041154	8.883251
6.834318	518.094066	8.888269
6.613580	510.496583	8.893287
6.593068	513.299561	8.898304
6.744070	511.653072	8.903322
6.798224	508.788398	8.908339
6.817522	514.410486	8.913357
6.657275	506.358023	8.918375
6.330756	512.991095	8.923392
6.576989	514.055759	8.928410
6.901442	512.996522	8.933427
6.528263	511.881248	8.938445
6.933658	500.108808	8.943463
6.741317	514.854519	8.948480
6.728538	510.405569	8.953498
6.646187	514.112280	8.958515
6.288447	502.041728	8.963533
6.586201	513.054554	8.968551
6.577206	516.265879	8.973568
6.410302	519.256795	8.978586
6.538887	510.121186	8.983603
6.374078	517.273189	8.988621
6.612428	516.889755	8.993639
6.504785	521.289185	8.998656
6.408733	548.305732	9.003674
6.928937	537.962219	9.008691
6.648003	546.315170	9.013709
6.987115	543.453289	9.018727
6.976796	552.496902	9.023744
6.832183	544.991820	9.028762
7.173678	538.838889	9.033779
6.941323	548.841245	9.038797
6.737247	523.971154	9.043815
6.867891	530.529767	9.048832
6.941210	532.427369	9.053850
6.887829	517.749952	9.058867
6.473488	521.921777	9.063885
6.878113	532.999027	9.068903
6.999638	534.242143	9.073920
6.826266	546.395621	9.078938
7.175432	537.228955	9.083955
7.363891	537.822954	9.088973
7.094379	513.245328	9.093991
6.735277	512.164434	9.099008
6.549438	515.785021	9.104026
6.695724	510.121942	9.109043
6.548341	531.368230	9.114061
7.103676	543.369007	9.119079
7.067286	540.893621	9.124096
7.082451	539.385498	9.129114
7.263690	525.090179	9.134131
6.801197	509.424987	9.139149
7.227243	511.963756	9.144167
7.129200	513.934743	9.149184
6.546047	516.868882	9.154202
6.969469	503.929923	9.159219
6.933717	509.735480	9.164237
7.024067	504.642061	9.169255
7.045239	510.613863	9.174272
6.862891	519.785274	9.179290
7.365389	524.471591	9.184307
7.226217	514.780155	9.189325
6.946105	503.393773	9.194343
6.905689	508.931456	9.199360
6.558884	508.352459	9.204378
6.883056	525.257531	9.209395
6.763569	530.702799	9.214413
6.808463	539.953377	9.219431
7.210761	551.687582	9.224448
6.913970	542.930845	9.229466
6.984080	542.675291	9.234483
6.572001	541.507204	9.239501
6.596891	546.949086	9.244519
6.964175	541.581296	9.249536
6.711519	553.963979	9.254554
7.401879	541.867012	9.259571
7.210424	553.037369	9.264589
7.107751	541.934859	9.269607
7.435948	549.554209	9.274624
7.623087	544.175842	9.279642
7.668757	533.119774	9.284659
7.496579	545.375788	9.289677
7.023523	545.714909	9.294695
6.833393	539.572584	9.299712
6.922056	542.775352	9.304730
7.220166	538.582435	9.309747
7.381035	540.482003	9.314765
7.445135	547.100527	9.319783
7.510399	543.027567	9.324800
7.352418	537.599760	9.329818
7.412209	542.774609	9.334835
7.208178	539.199306	9.339853
7.057652	549.580874	9.344871
7.289151	541.403726	9.349888
7.177348	542.540845	9.354906
7.328513	547.981442	9.359923
7.118717	543.255951	9.364941
7.347721	544.598113	9.369959
7.416964	543.105654	9.374976
7.102292	537.525924	9.379994
7.480896	535.416515	9.385011
7.189636	537.411268	9.390029
7.121081	541.896843	9.395047
7.318443	547.816025	9.400064
7.420686	542.241495	9.405082
7.391059	535.896404	9.410099
7.487895	540.428353	9.415117
7.367649	544.470892	9.420135
7.504352	534.516280	9.425152
7.543981	533.888577	9.430170
7.394110	505.969342	9.435187
6.856689	517.097752	9.440205
6.906767	529.018071	9.445223
6.911182	535.507211	9.450240
7.061411	543.641793	9.455258
7.083737	539.894269	9.460275
6.898535	547.330307	9.465293
7.044915	547.904395	9.470311
7.403316	542.285271	9.475328
7.069663	551.114654	9.480346
7.199443	566.317214	9.485363
7.383555	571.903231	9.490381
7.239850	577.370919	9.495399
7.609918	567.149127	9.500416
7.543551	581.711912	9.505434
7.396609	577.096963	9.510451
7.513002	573.362128	9.515469
7.532375	570.898777	9.520487
7.474317	572.873792	9.525504
7.345262	582.291499	9.530522
7.665943	566.861219	9.535539
7.483147	562.679670	9.540557
7.422220	582.394337	9.545575
7.870096	563.657197	9.550592
7.549546	570.488675	9.555610
7.504509	556.242430	9.560627
7.390765	555.216931	9.565645
7.233940	551.864780	9.570663
7.495201	564.919967	9.575680
7.156986	573.327271	9.580698
7.324596	570.753320	9.585715
7.459367	568.827281	9.590733
7.256631	569.347571	9.595751
7.573938	572.103098	9.600768
7.290542	573.025023	9.605786
7.454855	566.516204	9.610803
7.129075	571.070766	9.615821
7.217259	570.854046	9.620839
7.804154	590.205224	9.625856
7.263650	590.378953	9.630874
7.477807	599.868175	9.635891
7.733711	596.806201	9.640909
7.710840	604.778319	9.645927
8.104797	593.757053	9.650944
7.830082	580.248993	9.655962
7.852948	576.002358	9.660979
7.807331	565.503564	9.665997
7.454996	568.517950	9.671015
7.870695	568.560625	9.676032
8.032656	570.719018	9.681050
7.587950	569.875055	9.686067
7.667288	569.349427	9.691085
7.520112	571.465619	9.696103
7.625552	560.729113	9.701120
7.791739	570.516244	9.706138
8.067145	565.011003	9.711155
7.775339	568.787964	9.716173
7.709534	578.036292	9.721191
7.821069	559.978134	9.726208
7.607939	568.273838	9.731226
7.758652	568.024348	9.736243
7.898528	573.670224	9.741261
8.070978	565.995437	9.746279
7.853486	575.798938	9.751296
7.666342	569.276362	9.756314
7.921627	558.542550	9.761331
8.011036	568.907704	9.766349
7.860914	570.703681	9.771367
7.933426	567.447360	9.776384
8.046598	565.722686	9.781402
7.724804	574.120585	9.786419
7.813636	569.094901	9.791437
7.675470	577.330791	9.796455
7.955402	571.664596	9.801472
7.985562	569.439473	9.806490
7.842196	582.683269	9.811507
7.808366	571.226616	9.816525
7.719864	567.989818	9.821543
8.020339	568.824407	9.826560
8.070388	566.121489	9.831578
7.966777	575.253648	9.836595
8.172451	573.999708	9.841613
7.942975	563.375229	9.846631
8.188841	559.899553	9.851648
7.899772	564.950602	9.856666
7.567692	568.843939	9.861683
7.660998	563.098375	9.866701
7.638236	571.861633	9.871719
7.825432	564.804263	9.876736
7.839327	568.091031	9.881754
7.912585	573.907726	9.886771
7.883064	565.807551	9.891789
7.976374	579.827420	9.896807
7.796527	568.307023	9.901824
7.762861	574.778855	9.906842
7.703970	566.534548	9.911859
7.911254	568.899876	9.916877
7.594412	576.811133	9.921895
7.992476	592.411222	9.926912
7.924841	599.648858	9.931930
7.923321	609.072174	9.936947
8.533284	597.941898	9.941965
8.025326	596.311500	9.946983
7.985849	575.872076	9.952000
7.911140	598.292129	9.957018
7.911770	600.631486	9.962035
8.369689	607.496901	9.967053
7.969797	613.368872	9.972071
8.318315	594.665728	9.977088
8.347469	603.531032	9.982106
8.116001	598.795525	9.987123
8.018869	578.020814	9.992141
7.620563	579.896282	9.997159
7.889145	593.658406	10.002176
7.988931	607.114254	10.007194
8.099531	603.546083	10.012211
8.316152	611.536784	10.017229
8.112260	603.602287	10.022247
8.402905	604.346494	10.027264
8.460703	613.498547	10.032282
8.220061	607.993252	10.037299
8.436731	606.661819	10.042317
8.237113	607.239359	10.047335
8.316669	594.585941	10.052352
8.415998	594.065571	10.057370
7.998784	591.105878	10.062387
8.535403	595.758731	10.067405
8.501205	585.496274	10.072423
8.298853	579.056506	10.077440
8.323416	570.643910	10.082458
8.062008	569.817185	10.087475
8.007295	563.533795	10.092493
8.211503	575.662785	10.097511
8.249299	596.308009	10.102528
8.544357	596.103942	10.107546
8.088493	581.871147	10.112563
8.315522	580.148813	10.117581
8.446475	594.533166	10.122599
8.267512	591.557424	10.127616
8.349479	587.687653	10.132634
8.194920	596.205831	10.137651
8.444777	589.872492	10.142669
8.275153	595.706797	10.147687
8.455335	605.334878	10.152704
8.201865	605.235530	10.157722
8.340451	603.271365	10.162739
8.502804	595.907617	10.167757
8.354633	599.530856	10.172775
8.348640	604.570957	10.177792
8.175100	594.655374	10.182810
8.201542	603.803844	10.187827
8.614329	590.083462	10.192845
8.392231	599.849854	10.197863
8.450101	600.920363	10.202880
8.280613	601.447361	10.207898
8.382139	601.105035	10.212915
8.264854	594.602590	10.217933
8.296809	596.673045	10.222951
8.161163	602.365348	10.227968
8.219546	595.644640	10.232986
8.206066	595.446097	10.238003
8.530960	596.912153	10.243021
8.258039	601.731261	10.248039
8.588899	599.898183	10.253056
8.670553	594.589089	10.258074
8.172666	605.122173	10.263091
8.403943	619.286763	10.268109
8.363186	625.339991	10.273127
8.701255	627.254373	10.278144
8.821757	629.411753	10.283162
8.596230	628.747074	10.288179
8.916715	620.630852	10.293197
8.654269	607.664528	10.298215
8.754057	603.578269	10.303232
8.876948	597.971769	10.308250
8.372174	602.995497	10.313267
8.809480	585.290380	10.318285
8.761042	602.025467	10.323303
8.457331	598.646802	10.328320
8.984910	588.299085	10.333338
8.458771	596.994196	10.338355
8.514362	589.081281	10.343373
8.363425	592.431507	10.348391
8.236574	593.726695	10.353408
8.865380	608.894459	10.358426
8.759297	629.742208	10.363443
8.921190	620.845270	10.368461
9.093484	623.931796	10.373479
8.746675	614.424087	10.378496
8.925787	596.336711	10.383514
9.018057	600.453670	10.388531
9.042330	589.930714	10.393549
8.768880	592.679167	10.398567
8.749708	596.002010	10.403584
9.050056	590.974528	10.408602
8.863242	594.153750	10.413619
9.165891	586.596385	10.418637
8.600165	589.582469	10.423655
8.835200	594.546129	10.428672
8.773129	585.060858	10.433690
8.473422	593.155179	10.438707
8.633255	586.740281	10.443725
8.748496	590.810341	10.448743
8.625217	587.330124	10.453760
8.926784	596.398978	10.458778
8.558938	596.445376	10.463795
8.916486	593.717321	10.468813
8.895113	589.533888	10.473831
8.879804	592.106835	10.478848
9.055866	591.398131	10.483866
8.654076	594.721420	10.488883
8.758588	597.191317	10.493901
8.820996	592.024845	10.498919
8.711217	589.455597	10.503936
9.102991	608.212890	10.508954
8.937455	611.040344	10.513971
8.961995	604.894695	10.518989
9.028140	608.417080	10.524007
8.898194	599.412705	10.529024
9.173200	591.646858	10.534042
8.540637	601.193444	10.539059
8.897198	617.817633	10.544077
9.290982	624.921560	10.549095
8.915333	624.352246	10.554112
9.000712	629.025063	10.559130
8.833098	634.044057	10.564147
9.013175	619.598282	10.569165
8.984971	627.040396	10.574183
9.028398	617.470755	10.579200
9.055797	622.299480	10.584218
8.684288	622.472048	10.589235
9.102618	628.099187	10.594253
8.978500	623.658369	10.599271
8.847548	624.150757	10.604288
9.088139	615.593108	10.609306
8.852531	619.679628	10.614323
9.027676	621.635792	10.619341
9.215668	614.967558	10.624359
8.837850	627.888990	10.629376
8.881732	613.164804	10.634394
9.156913	619.163458	10.639411
8.929364	627.620501	10.644429
8.589949	626.361675	10.649447
8.648377	634.878430	10.654464
9.421761	644.960758	10.659482
9.216230	648.755954	10.664499
9.285503	658.700172	10.669517
9.580677	653.541169	10.674535
9.268913	654.707798	10.679552
9.883913	634.359215	10.684570
9.538071	631.674474	10.689587
9.066831	618.729261	10.694605
9.387015	614.579910	10.699623
9.313580	608.601699	10.704640
9.437368	611.520585	10.709658
9.386350	621.961431	10.714675
9.510919	615.087088	10.719693
9.583840	614.082105	10.724711
9.335202	616.225599	10.729728
9.567183	617.208491	10.734746
9.632842	621.466735	10.739763
9.259448	608.868181	10.744781
9.469837	610.040233	10.749799
9.148442	612.407912	10.754816
9.505496	616.171142	10.759834
9.405281	615.372391	10.764851
9.211124	608.311795	10.769869
9.235481	614.880038	10.774887
9.090578	610.361769	10.779904
9.440501	609.941887	10.784922
9.419637	605.306586	10.789939
9.411143	609.990384	10.794957
9.624132	612.324663	10.799975
9.118931	623.730839	10.804992
9.528772	612.565133	10.810010
9.447763	605.945195	10.815027
9.375852	619.341256	10.820045
9.269492	622.113568	10.825063
9.013183	619.618027	10.830080
9.600006	618.680844	10.835098
9.457916	608.305618	10.840115
9.329542	619.879000	10.845133
9.679050	609.247078	10.850151
9.440292	618.422064	10.855168
9.675194	617.530737	10.860186
9.574484	612.379897	10.865203
9.681924	609.775143	10.870221
10.016154	616.871294	10.875239
9.375688	627.864087	10.880256
9.187649	611.215239	10.885274
9.702756	612.432879	10.890291
9.467847	610.994120	10.895309
9.840663	610.647309	10.900327
9.804538	611.595781	10.905344
9.510987	615.461311	10.910362
9.645053	624.811650	10.915379
9.056026	617.179424	10.920397
10.224113	628.090428	10.925415
9.827458	627.457964	10.930432
9.691913	614.499201	10.935450
9.763460	616.214072	10.940467
9.650821	618.295139	10.945485
9.765989	605.894929	10.950503
9.650303	623.754116	10.955520
9.994309	611.892346	10.960538
9.843023	607.158444	10.965555
9.560512	615.344207	10.970573
9.892438	606.477435	10.975591
9.762967	610.465720	10.980608
9.536156	615.252414	10.985626
9.541015	603.530537	10.990643
9.710500	614.700729	10.995661
9.599199	616.667326	11.000679
9.700606	621.291242	11.005696
9.891154	631.160982	11.010714
10.060131	644.376537	11.015731
9.824094	625.194284	11.020749
9.696206	616.578556	11.025767
9.617770	625.831067	11.030784
9.808860	630.414283	11.035802
10.044609	641.633079	11.040819
10.125167	641.812717	11.045837
10.022126	628.393543	11.050855
9.828993	618.505586	11.055872
9.557007	616.802143	11.060890
9.835772	629.171756	11.065907
9.936867	639.688539	11.070925
10.029806	645.662607	11.075943
9.694664	648.130279	11.080960
10.093356	642.379387	11.085978
10.006641	635.793738	11.090995
10.118458	648.880779	11.096013
10.173892	632.916133	11.101031
10.018912	631.228877	11.106048
9.876220	624.953210	11.111066
9.978663	628.326126	11.116083
9.944751	649.199566	11.121101
10.187119	634.446495	11.126119
9.904782	642.685678	11.131136
9.621048	635.184156	11.136154
9.895755	641.264967	11.141171
9.486311	643.109317	11.146189
10.096685	631.364111	11.151207
9.686487	643.916573	11.156224
9.936416	639.389632	11.161242
10.076359	648.126636	11.166259
9.952288	646.481997	11.171277
10.317265	637.606005	11.176295
10.145086	645.076644	11.181312
9.910382	654.486564	11.186330
9.953471	644.152056	11.191347
9.950243	644.365614	11.196365
10.136206	643.962887	11.201383
10.295013	642.613559	11.206400
9.907559	645.256968	11.211418
10.054976	657.657856	11.216435
10.164120	677.662980	11.221453
10.365589	677.683590	11.226471
10.354055	668.476867	11.231488
10.140287	673.908834	11.236506
10.418646	671.589049	11.241523
10.301196	670.435735	11.246541
10.464650	670.656387	11.251559
10.001979	651.740248	11.256576
10.108945	652.723136	11.261594
10.725842	658.842268	11.266611
10.293810	659.830190	11.271629
10.234361	642.226484	11.276647
10.059559	647.292724	11.281664
9.809477	663.103124	11.286682
10.548192	661.627751	11.291699
10.389953	670.297335	11.296717
10.683245	667.035998	11.301735
10.290158	663.864472	11.306752
10.498826	671.153017	11.311770
10.842595	667.625516	11.316787
10.032530	658.152906	11.321805
10.611736	658.878361	11.326823
10.280879	652.937851	11.331840
10.162502	664.988751	11.336858
10.380197	668.485220	11.341875
10.501727	676.739750	11.346893
10.234462	672.026668	11.351911
10.335641	665.515939	11.356928
10.424915	670.347148	11.361946
10.607286	661.356664	11.366963
10.355266	671.810685	11.371981
10.489302	671.959147	11.376999
10.716887	656.645913	11.382016
10.571661	663.456233	11.387034
10.721442	667.492166	11.392051
10.570591	664.331485	11.397069
10.747436	661.480555	11.402087
10.545176	664.463270	11.407104
10.519825	668.539362	11.412122
10.779517	658.788022	11.417139
10.612065	667.386799	11.422157
10.683405	665.269696	11.427175
10.669350	660.841579	11.432192
10.534374	658.819288	11.437210
10.865896	665.237107	11.442227
10.698256	650.522353	11.447245
10.566835	647.259665	11.452263
10.383238	652.258378	11.457280
10.418982	667.721609	11.462298
11.126742	657.984789	11.467315
10.739546	670.120168	11.472333
10.714252	672.516074	11.477351
10.566567	661.050221	11.482368
10.474631	678.638277	11.487386
10.524157	668.118573	11.492403
10.292245	670.427092	11.497421
10.433596	664.914053	11.502439
10.566568	664.441850	11.507456
10.580116	673.357894	11.512474
10.729204	662.179742	11.517491
10.770466	670.240882	11.522509
10.754504	665.192335	11.527527
10.990615	663.747668	11.532544
10.716972	666.783018	11.537562
10.992283	665.894359	11.542579
10.786199	667.973064	11.547597
10.728632	673.029190	11.552615
10.803989	674.711259	11.557632
10.843820	679.837298	11.562650
10.876899	666.175561	11.567667
10.420601	665.981312	11.572685
11.100500	679.005793	11.577703
10.897444	675.540806	11.582720
10.814102	692.862649	11.587738
11.143835	686.047856	11.592755
11.036473	676.306286	11.597773
10.667714	667.203962	11.602791
10.923108	679.910287	11.607808
10.828383	699.810476	11.612826
11.049164	697.357613	11.617843
10.557992	709.504399	11.622861
11.104817	690.733433	11.627879
11.137491	691.396579	11.632896
10.886691	700.320897	11.637914
11.207371	696.381047	11.642931
11.091128	693.398856	11.647949
11.267089	695.078276	11.652967
11.428747	691.961202	11.657984
11.096198	694.322963	11.663002
11.463294	686.703826	11.668019
11.173757	675.553669	11.673037
10.883667	665.243504	11.678055
10.921335	672.051453	11.683072
10.915180	687.859848	11.688090
11.607856	690.775763	11.693107
11.228640	673.918132	11.698125
10.822738	672.623153	11.703143
11.310010	675.843329	11.708160
11.445300	685.892479	11.713178
11.325550	677.380960	11.718195
10.893572	673.181812	11.723213
11.226747	685.069148	11.728231
11.164112	689.831194	11.733248
11.147370	690.111540	11.738266
11.262054	688.649936	11.743283
11.527774	694.002772	11.748301
11.229669	684.993366	11.753319
11.424485	685.209623	11.758336
11.524099	669.273557	11.763354
11.167664	661.905666	11.768371
11.144211	662.148250	11.773389
10.898875	680.012986	11.778407
11.061747	684.942547	11.783424
10.854940	687.160126	11.788442
11.275061	692.632692	11.793459
11.354452	699.682135	11.798477
11.270040	695.028968	11.803495
11.496087	695.439139	11.808512
11.179076	705.509021	11.813530
11.464606	690.412019	11.818547
11.629803	687.035554	11.823565
11.515782	686.744986	11.828583
11.797566	687.529728	11.833600
11.346784	686.629588	11.838618
11.449150	682.785255	11.843635
11.464858	684.920698	11.848653
11.319854	692.669293	11.853671
11.631001	680.533427	11.858688
11.394813	690.913994	11.863706
11.303685	689.739894	11.868723
11.575973	687.053565	11.873741
11.331845	686.504926	11.878759
11.621536	676.265937	11.883776
11.197870	687.534891	11.888794
11.140213	689.856932	11.893811
11.320470	690.446978	11.898829
11.314302	696.390700	11.903847
11.841569	705.980381	11.908864
11.767169	708.796630	11.913882
11.826997	703.714979	11.918899
11.863308	698.230407	11.923917
11.732846	687.772119	11.928935
11.595671	674.410799	11.933952
11.524605	682.381672	11.938970
11.609712	680.133774	11.943987
11.932650	685.210865	11.949005
11.557258	690.301214	11.954023
11.914760	694.350948	11.959040
11.667563	686.971585	11.964058
11.835420	687.536915	11.969075
11.761720	682.277868	11.974093
11.494154	692.047798	11.979111
11.730396	696.146502	11.984128
11.924726	705.071264	11.989146
11.995888	710.240453	11.994163
11.809180	684.555382	11.999181
11.844297	691.722352	12.004199
11.685181	683.224125	12.009216
11.608447	690.533274	12.014234
12.079515	702.364772	12.019251
12.151144	717.030939	12.024269
11.911037	712.939907	12.029287
11.760914	686.670947	12.034304
11.803877	688.326291	12.039322
11.771901	698.295729	12.044339
12.047592	707.037692	12.049357
11.941594	713.404137	12.054375
11.889752	710.421731	12.059392
12.045930	712.421290	12.064410
12.037444	709.439100	12.069427
12.131677	703.569240	12.074445
11.645141	697.206693	12.079463
11.795889	713.490661	12.084480
11.819791	710.864269	12.089498
11.871576	704.256392	12.094515
12.044068	706.728062	12.099533
12.058301	711.735236	12.104551
12.138642	704.272511	12.109568
11.841809	709.916014	12.114586
11.926704	711.817235	12.119603
12.145283	701.222632	12.124621
12.016448	714.447706	12.129639
12.072017	705.295903	12.134656
12.374432	708.624276	12.139674
12.107914	705.964201	12.144691
12.504959	711.008684	12.149709
12.150460	706.443642	12.154727
12.266967	709.556231	12.159744
12.311575	712.229118	12.164762
11.882853	713.934662	12.169779
12.337011	704.512700	12.174797
12.378309	709.966493	12.179815
12.289957	709.368985	12.184832
12.396335	702.636461	12.189850
12.165207	708.218622	12.194867
12.450695	709.769631	12.199885
12.346713	718.184360	12.204903
12.558821	704.958956	12.209920
12.360405	709.766769	12.214938
12.086893	699.208220	12.219955
12.465157	704.008215	12.224973
12.364903	708.687328	12.229991
12.430590	702.700163	12.235008
12.283458	681.145245	12.240026
12.261959	696.604483	12.245043
12.555935	698.690498	12.250061
12.241895	709.356624	12.255079
12.492687	702.253748	12.260096
12.289290	701.852087	12.265114
12.129522	713.474616	12.270131
12.748777	702.319309	12.275149
12.399324	704.139877	12.280167
12.663502	706.411392	12.285184
12.412271	708.650092	12.290202
12.328784	704.825544	12.295219
12.429562	706.577023	12.300237
12.363451	706.082808	12.305255
12.269019	711.825121	12.310272
12.565052	706.330690	12.315290
12.498629	708.220605	12.320307
12.336087	704.912861	12.325325
12.261371	712.672287	12.330343
12.344088	703.841328	12.335360
12.250698	705.774865	12.340378
12.542843	717.967669	12.345395
12.607294	701.735963	12.350413
12.231455	714.517994	12.355431
12.465929	721.294721	12.360448
12.883346	732.465160	12.365466
12.350472	735.720100	12.370483
12.531293	743.431803	12.375501
12.407495	745.516700	12.380519
13.053529	736.201960	12.385536
13.107917	743.188539	12.390554
12.881546	738.054389	12.395571
12.923692	729.150804	12.400589
12.672172	719.390125	12.405607
12.478617	705.990072	12.410624
12.622414	724.196478	12.415642
12.785053	734.584380	12.420659
12.784720	726.264575	12.425677
13.042445	726.195096	12.430695
12.994575	730.269416	12.435712
12.926636	733.181827	12.440730
12.940112	723.073475	12.445747
13.154106	701.887900	12.450765
12.524377	704.247503	12.455783
12.978061	697.778488	12.460800
12.971064	699.874091	12.465818
12.647838	697.990363	12.470835
12.763096	695.980051	12.475853
12.952511	710.760186	12.480871
12.846319	726.667912	12.485888
12.894537	724.189438	12.490906
13.333518	727.881787	12.495923
13.173783	721.595120	12.500941
13.138657	710.504844	12.505959
12.735576	687.388591	12.510976
13.055619	701.640834	12.515994
13.241225	720.917181	12.521011
13.054967	706.346368	12.526029
12.781236	701.856250	12.531047
12.776067	721.273060	12.536064
13.199259	721.781041	12.541082
13.338888	731.635939	12.546099
13.218744	736.156666	12.551117
13.321775	722.377336	12.556135
13.356953	712.232242	12.561152
13.217007	703.386908	12.566170
12.327866	712.940930	12.571187
12.756422	714.567392	12.576205
13.294258	732.705149	12.581223
13.122351	726.685007	12.586240
13.435337	728.669971	12.591258
13.170255	728.932411	12.596275
13.033574	730.766138	12.601293
12.926621	734.433079	12.606311
12.995785	725.410684	12.611328
13.095963	722.651334	12.616346
13.547962	729.259860	12.621363
13.460261	725.442104	12.626381
13.276184	731.801385	12.631399
13.194055	728.469424	12.636416
13.400108	726.013578	12.641434
13.186132	727.609536	12.646451
13.251903	720.221048	12.651469
13.189334	725.519308	12.656487
12.788662	734.148987	12.661504
13.092287	735.329061	12.666522
13.383770	754.586184	12.671539
13.377345	751.352513	12.676557
13.593590	753.545162	12.681575
13.670667	760.276966	12.686592
13.865901	753.805764	12.691610
13.354322	746.793622	12.696627
13.319227	716.523598	12.701645
13.325592	739.192613	12.706663
13.167398	756.401429	12.711680
13.642818	759.412501	12.716698
13.399171	758.767932	12.721715
13.525217	759.865761	12.726733
13.509704	764.661276	12.731751
13.447337	755.303089	12.736768
13.804341	760.112520	12.741786
13.352796	756.213473	12.746803
13.649059	755.474959	12.751821
13.703535	753.399699	12.756839
13.492213	761.177985	12.761856
13.732252	751.555105	12.766874
13.886118	768.539761	12.771891
13.360645	755.154563	12.776909
13.395235	761.526531	12.781927
13.550509	761.070419	12.786944
13.926981	756.792361	12.791962
13.530878	762.004933	12.796979
13.627807	754.921259	12.801997
13.635790	752.177828	12.807015
13.507260	766.853699	12.812032
13.817771	745.163528	12.817050
13.732844	755.638902	12.822067
13.933978	752.984100	12.827085
13.602695	749.911179	12.832103
13.269761	763.053018	12.837120
14.105826	773.545662	12.842138
14.097213	779.365631	12.847155
14.272603	773.624137	12.852173
14.149353	755.743301	12.857191
14.188905	746.944347	12.862208
13.891555	753.364768	12.867226
13.644587	754.563306	12.872243
13.812883	758.292522	12.877261
13.917496	757.107031	12.882279
13.597646	763.816848	12.887296
13.806607	757.912558	12.892314
13.900429	773.394934	12.897331
14.327405	784.118642	12.902349
14.489074	777.800981	12.907367
14.157722	760.481199	12.912384
14.102506	753.044002	12.917402
13.927698	764.171906	12.922419
14.048659	752.247399	12.927437
13.885586	749.102791	12.932455
14.214975	756.850469	12.937472
14.032994	750.465912	12.942490
13.661742	755.335365	12.947507
14.256287	774.612496	12.952525
14.707261	779.909359	12.957543
14.335821	773.262358	12.962560
14.328495	756.723618	12.967578
14.032212	756.744216	12.972595
14.026856	746.149587	12.977613
14.173024	753.114017	12.982631
13.994934	749.763664	12.987648
14.161588	757.576515	12.992666
14.289167	780.906925	12.997683
14.395513	773.587183	13.002701
14.674376	779.762030	13.007719
14.608787	777.517569	13.012736
14.143299	755.197793	13.017754
13.949254	750.829506	13.022771
14.054004	764.103112	13.027789
14.489448	773.796379	13.032807
14.469885	783.771398	13.037824
14.242595	778.431815	13.042842
14.578672	778.278143	13.047859
14.433889	786.646512	13.052877
14.266345	778.476925	13.057895
14.299297	778.083342	13.062912
14.466134	772.863141	13.067930
14.701861	783.806803	13.072947
14.621003	774.721294	13.077965
14.586779	775.020276	13.082983
14.420716	795.220807	13.088000
14.616542	767.445406	13.093018
14.673492	783.306944	13.098035
14.720758	773.662176	13.103053
14.854758	782.799966	13.108071
14.474548	774.134131	13.113088
14.378912	754.911883	13.118106
14.095686	769.909130	13.123123
14.381803	769.238028	13.128141
14.673966	775.670664	13.133159
14.404887	775.289303	13.138176
14.723461	776.784172	13.143194
14.483090	775.318451	13.148211
14.046737	783.476488	13.153229
14.414327	778.945315	13.158247
14.524567	778.161866	13.163264
14.637893	775.254397	13.168282
14.811728	782.393369	13.173299
14.566653	796.026919	13.178317
15.058182	793.133016	13.183335
14.772520	789.178010	13.188352
14.908281	782.891099	13.193370
15.000721	777.189684	13.198387
14.549792	778.091677	13.203405
15.058485	781.399264	13.208423
14.647701	785.254195	13.213440
14.911797	786.698040	13.218458
14.700615	796.813669	13.223475
14.825240	801.022562	13.228493
14.614292	798.983678	13.233511
14.953834	803.786463	13.238528
14.989762	796.969987	13.243546
15.061652	809.329355	13.248563
15.139276	799.289078	13.253581
15.247829	803.295449	13.258599
15.418882	797.110554	13.263616
14.972061	801.991624	13.268634
15.018340	783.956780	13.273651
14.978215	800.211666	13.278669
15.413291	797.709302	13.283687
14.650225	787.467276	13.288704
14.926877	790.616004	13.293722
15.183771	795.956459	13.298739
14.829557	796.054333	13.303757
15.066875	795.977501	13.308775
14.919114	810.132183	13.313792
14.978495	798.075718	13.318810
15.004035	793.605100	13.323827
15.120315	812.370087	13.328845
15.361395	797.027914	13.333863
14.762473	809.459856	13.338880
15.239330	799.459686	13.343898
15.084848	797.328318	13.348915
15.139964	801.619550	13.353933
15.359506	803.284695	13.358951
15.011377	798.945203	13.363968
15.017048	798.749299	13.368986
15.532300	822.096892	13.374003
15.322567	823.956282	13.379021
15.519799	822.751839	13.384039
15.616303	821.734384	13.389056
15.427679	813.296070	13.394074
15.700414	795.912635	13.399091
15.582773	801.739903	13.404109
15.681854	787.250969	13.409127
15.274079	798.343198	13.414144
15.318071	782.817114	13.419162
15.713133	789.283628	13.424179
15.384789	800.885074	13.429197
15.696403	792.837342	13.434215
15.416639	791.104854	13.439232
15.430704	797.961633	13.444250
15.645533	797.201738	13.449267
15.685762	794.391467	13.454285
15.584868	788.876790	13.459303
15.650122	788.012209	13.464320
15.708508	798.191146	13.469338
15.474474	791.906003	13.474355
15.228733	799.532250	13.479373
15.696859	788.731419	13.484391
15.436143	797.361032	13.489408
15.653060	808.424923	13.494426
16.168041	822.939595	13.499443
15.571996	806.771857	13.504461
15.701322	787.913890	13.509479
15.558051	806.744494	13.514496
15.703009	817.776296	13.519514
15.754059	817.067575	13.524531
16.042565	819.477679	13.529549
15.920978	815.658218	13.534567
15.377751	802.695026	13.539584
15.557272	820.672752	13.544602
15.585802	814.223268	13.549619
15.561904	822.793193	13.554637
15.606273	822.639211	13.559655
15.548190	827.198519	13.564672
15.492555	824.222327	13.569690
15.553026	819.762265	13.574707
15.518995	847.513043	13.579725
15.925138	855.048223	13.584743
16.334746	848.406837	13.589760
16.134428	850.031155	13.594778
16.051338	852.297984	13.599795
16.179248	856.633196	13.604813
16.579558	842.396146	13.609831
16.170092	829.898431	13.614848
16.092660	824.550108	13.619866
16.188555	817.758647	13.624883
15.703139	828.815017	13.629901
16.178697	819.192832	13.634919
15.859813	811.677547	13.639936
16.059682	827.843896	13.644954
16.176961	843.184598	13.649971
16.086204	845.907628	13.654989
16.159159	836.564917	13.660007
16.708720	847.159770	13.665024
16.316999	835.199865	13.670042
16.366407	830.599528	13.675059
16.114995	825.132640	13.680077
16.040538	821.653749	13.685095
16.155218	838.381918	13.690112
16.375717	842.424809	13.695130
16.404758	841.579002	13.700147
16.376526	854.164559	13.705165
16.500618	847.384072	13.710183
16.630012	846.282848	13.715200
16.447543	839.677214	13.720218
16.221150	819.579515	13.725235
16.410362	831.166014	13.730253
16.541852	832.948548	13.735271
16.222369	829.527860	13.740288
16.284133	838.097513	13.745306
16.509804	834.943065	13.750323
16.478338	858.486652	13.755341
16.594294	839.797434	13.760359
16.926629	845.959436	13.765376
16.419399	841.592690	13.770394
16.551452	841.563661	13.775411
16.418204	849.671840	13.780429
16.764929	849.018174	13.785447
16.809712	850.470418	13.790464
16.238077	842.597158	13.795482
16.803619	838.227018	13.800499
16.514636	850.459378	13.805517
16.455850	848.749607	13.810535
16.885371	847.654288	13.815552
16.698780	847.612376	13.820570
16.744836	838.845360	13.825587
16.530249	843.910170	13.830605
16.499938	837.961744	13.835623
16.936747	839.855506	13.840640
16.775285	847.979270	13.845658
16.744644	839.980003	13.850675
16.748677	860.442122	13.855693
16.734080	845.034102	13.860711
16.953192	842.250648	13.865728
16.611361	846.859804	13.870746
16.845846	840.237619	13.875763
16.479198	853.428897	13.880781
16.743585	838.172873	13.885799
16.872882	838.494135	13.890816
16.681000	851.890150	13.895834
16.594790	847.722772	13.900851
16.739266	861.079841	13.905869
16.668565	879.017997	13.910887
16.920813	879.284302	13.915904
17.026714	884.439346	13.920922
17.176344	879.465511	13.925939
17.222656	891.676248	13.930957
17.357535	879.714013	13.935975
17.425206	872.317561	13.940992
16.997081	867.040756	13.946010
17.186291	858.860194	13.951027
17.069927	861.794900	13.956045
16.966513	881.780211	13.961063
17.327642	883.859780	13.966080
17.058226	882.389106	13.971098
17.336417	870.774485	13.976115
17.059778	884.712291	13.981133
17.353911	870.946023	13.986151
17.197247	882.961598	13.991168
17.053302	878.893402	13.996186
17.353988	880.392123	14.001203
17.624945	882.289484	14.006221
17.237021	881.156642	14.011239
17.595732	881.796818	14.016256
17.709378	882.873186	14.021274
17.509137	865.243385	14.026291
17.215239	855.264171	14.031309
17.365399	860.328739	14.036327
17.649393	862.883466	14.041344
17.181645	862.790298	14.046362
17.298136	860.829850	14.051379
17.324514	867.526584	14.056397
17.513462	871.543108	14.061415
17.634231	876.494549	14.066432
17.299824	863.793887	14.071450
17.834187	862.980792	14.076467
17.696092	874.922931	14.081485
17.529879	873.661244	14.086503
17.406504	871.910677	14.091520
17.542351	870.919191	14.096538
17.713261	877.073046	14.101555
17.527628	872.070774	14.106573
17.585976	874.655017	14.111591
17.741609	865.368986	14.116608
17.592424	877.850065	14.121626
17.357658	870.437758	14.126643
17.789591	879.404445	14.131661
17.818737	871.703787	14.136679
17.955752	863.202283	14.141696
17.646673	875.266067	14.146714
17.599363	869.242303	14.151731
17.767570	874.388326	14.156749
17.811821	881.111536	14.161767
18.161158	868.852599	14.166784
17.773213	876.038592	14.171802
17.800090	878.790999	14.176819
18.023059	868.253911	14.181837
17.516928	872.421513	14.186855
18.052434	869.239377	14.191872
17.916941	873.093219	14.196890
17.845517	874.266299	14.201907
17.756592	869.110473	14.206925
17.767698	872.798087	14.211943
17.898578	864.981820	14.216960
17.872201	869.972434	14.221978
18.014908	883.141365	14.226995
17.731930	899.666073	14.232013
17.712763	893.734580	14.237031
17.906791	894.836536	14.242048
17.397955	893.217566	14.247066
17.995249	895.276217	14.252083
18.191989	895.139862	14.257101
17.833148	902.238986	14.262119
18.176310	892.318222	14.267136
18.152232	896.377435	14.272154
18.062102	898.149955	14.277171
18.411016	904.388656	14.282189
18.593454	921.141538	14.287207
18.432462	896.342251	14.292224
18.265194	899.547730	14.297242
18.111820	906.576393	14.302259
18.155890	901.136717	14.307277
18.291490	910.406284	14.312295
18.879190	912.016998	14.317312
18.347557	916.233208	14.322330
18.425340	900.850606	14.327347
18.215388	899.847181	14.332365
18.454910	904.092911	14.337383
18.666383	909.379899	14.342400
18.640662	916.565786	14.347418
18.513675	900.515675	14.352435
18.249133	901.861195	14.357453
18.379464	902.211417	14.362471
18.902291	920.478133	14.367488
18.696408	911.395294	14.372506
18.518966	905.459741	14.377523
18.673690	901.379676	14.382541
18.555284	901.984644	14.387559
18.700693	891.289423	14.392576
18.743861	910.177911	14.397594
18.710522	907.540968	14.402611
18.714491	896.848254	14.407629
18.402968	908.148730	14.412647
19.015016	916.559098	14.417664
18.771407	925.729950	14.422682
18.755747	909.700205	14.427699
18.771600	914.167315	14.432717
18.954098	916.477848	14.437735
18.783689	918.064362	14.442752
18.850841	934.098550	14.447770
18.596999	920.507128	14.452787
18.573637	920.929097	14.457805
18.528193	930.893335	14.462823
18.883933	921.051069	14.467840
18.596750	921.303781	14.472858
18.514290	932.501275	14.477875
18.708804	922.663706	14.482893
18.653873	913.517935	14.487911
18.872158	926.661030	14.492928
18.652759	946.029289	14.497946
18.912203	949.428487	14.502963
19.094639	946.094582	14.507981
18.752055	952.793477	14.512999
19.170021	949.125032	14.518016
18.993386	956.317966	14.523034
18.922345	950.531220	14.528051
19.386248	949.333576	14.533069
18.906302	956.553114	14.538087
19.312875	951.332107	14.543104
19.300751	953.224396	14.548122
19.380994	949.103782	14.553139
19.446518	953.254385	14.558157
19.365089	947.900184	14.563175
19.374964	949.306936	14.568192
19.285674	941.831880	14.573210
19.301331	945.640293	14.578227
19.321676	948.083808	14.583245
19.268654	949.756813	14.588263
19.137942	952.424271	14.593280
18.964436	953.918896	14.598298
19.121261	956.542972	14.603315
19.347444	944.964346	14.608333
19.172218	955.761612	14.613351
19.169664	950.807490	14.618368
19.420204	967.698453	14.623386
20.061279	980.288841	14.628403
19.966991	961.889881	14.633421
19.338065	953.426532	14.638439
19.440661	950.198421	14.643456
19.736979	949.710631	14.648474
19.655617	943.617873	14.653491
19.787119	946.341980	14.658509
19.361911	959.914613	14.663527
19.497010	946.984649	14.668544
19.592567	961.117565	14.673562
19.378171	977.688395	14.678579
19.925071	973.835675	14.683597
19.740032	987.063186	14.688615
19.868754	987.939566	14.693632
19.883447	979.175881	14.698650
19.733032	984.270873	14.703667
20.059815	976.212961	14.708685
19.734750	981.558329	14.713703
19.973293	975.490435	14.718720
19.718283	985.989939	14.723738
19.667905	985.569183	14.728755
19.964546	982.681373	14.733773
20.098107	988.344290	14.738791
19.986649	979.059619	14.743808
19.932180	981.647565	14.748826
19.720847	979.863597	14.753843
20.206785	976.216585	14.758861
20.123274	983.902123	14.763879
19.952965	979.914621	14.768896
19.817853	977.448787	14.773914
19.740509	978.979975	14.778931
20.398847	982.955765	14.783949
20.080246	982.332429	14.788967
20.113451	980.281024	14.793984
20.596031	988.419671	14.799002
20.019526	986.949152	14.804019
20.482736	983.617453	14.809037
20.009613	985.277911	14.814055
20.427103	977.231481	14.819072
20.435011	977.791664	14.824090
19.819000	971.761366	14.829107
20.261221	969.615210	14.834125
20.260409	972.545308	14.839143
20.260885	977.349859	14.844160
20.082680	982.136605	14.849178
20.277507	975.974476	14.854195
20.492842	967.759624	14.859213
20.473413	983.270078	14.864231
20.269025	972.557718	14.869248
20.391172	976.061584	14.874266
20.039735	975.442100	14.879283
20.256167	964.928562	14.884301
20.133051	974.581607	14.889319
20.042604	999.473500	14.894336
20.002309	1001.953811	14.899354
20.273917	1001.277520	14.904371
20.227292	999.953646	14.909389
20.359210	999.178610	14.914407
20.630733	992.253244	14.919424
20.527265	1009.448182	14.924442
20.552916	1020.756691	14.929459
21.085741	1025.158970	14.934477
20.898331	1016.146723	14.939495
20.238013	1008.999224	14.944512
20.612513	1009.964692	14.949530
20.701995	1025.970093	14.954547
20.919460	1024.733950	14.959565
20.863750	1028.565100	14.964583
20.492384	1029.757350	14.969600
21.049407	1017.268931	14.974618
21.132998	1037.735853	14.979635
21.019309	1019.712012	14.984653
21.370457	1030.548111	14.989671
21.271553	1022.013177	14.994688
21.404621	1006.101050	14.999706
20.937550	1005.603904	15.004723
21.112769	1003.640031	15.009741
21.018133	995.334680	15.014759
20.929883	996.168583	15.019776
21.113168	989.636769	15.024794
20.989575	997.143045	15.029811
20.814770	995.181710	15.034829
21.194242	1000.414890	15.039847
21.193448	1017.666873	15.044864
21.028485	1008.446724	15.049882
21.308939	1024.028804	15.054899
21.419147	1020.429898	15.059917
21.204185	1003.094545	15.064935
21.238350	1009.474657	15.069952
21.139242	1002.204996	15.074970
20.859767	1016.283915	15.079987
21.038355	1023.885124	15.085005
21.175562	1037.419698	15.090023
21.221518	1026.573230	15.095040
21.648709	1030.303127	15.100058
21.380571	1030.392780	15.105075
21.359274	1027.368067	15.110093
21.650600	1028.709225	15.115111
21.602928	1022.275198	15.120128
21.768435	1019.400982	15.125146
21.343038	1031.977231	15.130163
21.453644	1034.791800	15.135181
21.588806	1025.594375	15.140199
21.175293	1019.846877	15.145216
21.900306	1019.755090	15.150234
21.407101	1027.600167	15.155251
21.550530	1028.200447	15.160269
21.876785	1022.223139	15.165287
21.331265	1025.141803	15.170304
21.624892	1022.677933	15.175322
21.365005	1027.805889	15.180339
21.649775	1027.600665	15.185357
21.577254	1035.536239	15.190375
21.337385	1023.091035	15.195392
21.767379	1034.373771	15.200410
21.655909	1044.557519	15.205427
21.873354	1051.007146	15.210445
21.700884	1058.900794	15.215463
21.671348	1048.268621	15.220480
22.260774	1042.180308	15.225498
21.914148	1053.399698	15.230515
21.987898	1048.276269	15.235533
21.906672	1048.990630	15.240551
21.385205	1055.648177	15.245568
21.686614	1050.322589	15.250586
21.728218	1052.767233	15.255603
21.881849	1052.579350	15.260621
22.432625	1047.969213	15.265639
22.119144	1053.614804	15.270656
22.163753	1047.359480	15.275674
21.887815	1049.380992	15.280691
22.021611	1049.907680	15.285709
22.170203	1046.831270	15.290727
21.915810	1048.099155	15.295744
21.959454	1051.598495	15.300762
21.690251	1059.998398	15.305779
22.271517	1070.737650	15.310797
22.482302	1071.652925	15.315815
22.379436	1085.064545	15.320832
22.580027	1080.377842	15.325850
22.434314	1070.371736	15.330867
22.465950	1078.352904	15.335885
22.628937	1078.022259	15.340903
22.538493	1060.174715	15.345920
22.453785	1044.797564	15.350938
22.208788	1045.222803	15.355955
22.344149	1050.075940	15.360973
22.859222	1063.525558	15.365991
22.718569	1069.132557	15.371008
22.314157	1044.808024	15.376026
22.615807	1054.427730	15.381043
22.846262	1071.781496	15.386061
22.940226	1058.993350	15.391079
22.366562	1043.957488	15.396096
22.592093	1040.708058	15.401114
22.599103	1054.428897	15.406131
22.529063	1057.967789	15.411149
22.472564	1060.122892	15.416167
22.347405	1077.653618	15.421184
22.746443	1062.175353	15.426202
22.663353	1069.860077	15.431219
22.568208	1068.384498	15.436237
22.965948	1066.673559	15.441255
22.892696	1070.932742	15.446272
22.826298	1063.849248	15.451290
23.007712	1062.706839	15.456307
22.759788	1070.435434	15.461325
23.086696	1063.153110	15.466343
22.915766	1075.090596	15.471360
23.220521	1074.585171	15.476378
23.154725	1073.287782	15.481395
23.158840	1072.898268	15.486413
23.172826	1073.178463	15.491431
23.170138	1076.718333	15.496448
23.464296	1067.077653	15.501466
23.083648	1075.945510	15.506483
22.974635	1076.984585	15.511501
23.363911	1071.516735	15.516519
23.039336	1078.342410	15.521536
23.100436	1071.976987	15.526554
22.964405	1073.770201	15.531571
22.929615	1073.647701	15.536589
23.091654	1066.781923	15.541607
22.696625	1064.912474	15.546624
23.113157	1079.377332	15.551642
23.103551	1097.545762	15.556659
22.769635	1095.882315	15.561677
23.031611	1093.862173	15.566695
23.186737	1101.616485	15.571712
23.040752	1105.734376	15.576730
23.219513	1103.509714	15.581747
23.115966	1112.848444	15.586765
23.228814	1121.198826	15.591783
23.466916	1138.130214	15.596800
23.550311	1137.210656	15.601818
23.353137	1127.040606	15.606835
23.365147	1129.997547	15.611853
23.854646	1133.727211	15.616871
23.733888	1141.078981	15.621888
24.102082	1135.983723	15.626906
24.015282	1132.387234	15.631923
23.623528	1139.583623	15.636941
23.806549	1128.355044	15.641959
24.011240	1128.301317	15.646976
23.885991	1121.730192	15.651994
23.953911	1127.036156	15.657011
23.967476	1129.229977	15.662029
24.102614	1118.159293	15.667047
23.736980	1108.740986	15.672064
23.765137	1117.847755	15.677082
24.101895	1129.449362	15.682099
23.661159	1127.307191	15.687117
23.625768	1123.630961	15.692135
23.923538	1128.609424	15.697152
24.009936	1132.707619	15.702170
24.224028	1125.426195	15.707187
24.194824	1126.088958	15.712205
24.247914	1125.481837	15.717223
23.945901	1131.925131	15.722240
24.055276	1132.142820	15.727258
24.204207	1118.032377	15.732275
24.107203	1140.418822	15.737293
24.245498	1136.045889	15.742311
24.106556	1130.766570	15.747328
24.012660	1134.411963	15.752346
24.361299	1127.693835	15.757363
24.027261	1126.849952	15.762381
24.101183	1128.803523	15.767399
23.858894	1127.034198	15.772416
23.943395	1129.540848	15.777434
24.284653	1137.194352	15.782451
24.335552	1160.317280	15.787469
24.319326	1152.797769	15.792487
24.459569	1159.185507	15.797504
24.743766	1146.461899	15.802522
24.713851	1148.201765	15.807539
24.242704	1152.271648	15.812557
24.431454	1150.220889	15.817575
24.665281	1151.947875	15.822592
24.556291	1148.484555	15.827610
24.674960	1154.394442	15.832627
24.529610	1153.082834	15.837645
24.682081	1147.960043	15.842663
24.635401	1146.719124	15.847680
24.229764	1155.495502	15.852698
24.719004	1150.053322	15.857715
24.457321	1157.577379	15.862733
24.691207	1147.413824	15.867751
24.580665	1154.593862	15.872768
24.670976	1170.622895	15.877786
24.957973	1181.721629	15.882803
25.043545	1179.417293	15.887821
25.436129	1171.496807	15.892839
25.199558	1156.276607	15.897856
24.831390	1152.927757	15.902874
24.848491	1144.980963	15.907891
24.922544	1160.448987	15.912909
25.127385	1165.592204	15.917927
25.401371	1178.865953	15.922944
25.431033	1158.265632	15.927962
25.203605	1144.500777	15.932979
24.822064	1148.019524	15.937997
25.608550	1139.962122	15.943015
25.032903	1156.937272	15.948032
25.121733	1140.128926	15.953050
25.593876	1143.374928	15.958067
24.897342	1153.121859	15.963085
24.877600	1147.102681	15.968103
25.387891	1159.517619	15.973120
25.196452	1178.926524	15.978138
25.669258	1183.718429	15.983155
25.692013	1187.934618	15.988173
25.345194	1174.879509	15.993191
24.965117	1165.655450	15.998208
25.308749	1174.181074	16.003226
25.560186	1173.782866	16.008243
25.571400	1181.134497	16.013261
25.297505	1174.310400	16.018279
25.683145	1179.781756	16.023296
25.503997	1178.972106	16.028314
25.785276	1170.033374	16.033331
25.543811	1176.899090	16.038349
25.804511	1172.991075	16.043367
25.372758	1183.382541	16.048384
25.338286	1179.588842	16.053402
25.369615	1174.640760	16.058419
25.467003	1190.791459	16.063437
25.833310	1193.026194	16.068455
26.155257	1190.399770	16.073472
25.673253	1187.951272	16.078490
25.836120	1182.385683	16.083507
25.559767	1188.534453	16.088525
25.887652	1197.001285	16.093543
25.980134	1192.201726	16.098560
25.733356	1202.013909	16.103578
26.318286	1191.915325	16.108595
26.132901	1202.787660	16.113613
26.241323	1195.522091	16.118631
26.224888	1195.333870	16.123648
26.427624	1197.929046	16.128666
26.306785	1184.990889	16.133683
26.106450	1174.503271	16.138701
26.033724	1166.482939	16.143719
26.353760	1176.957415	16.148736
26.272092	1185.993412	16.153754
26.297108	1180.404547	16.158771
25.738300	1181.110743	16.163789
25.947191	1193.194476	16.168807
26.295322	1190.760937	16.173824
26.252534	1192.869803	16.178842
26.341756	1185.993962	16.183859
26.452406	1198.314173	16.188877
26.268985	1192.496997	16.193895
26.365801	1184.319525	16.198912
25.897886	1191.137840	16.203930
26.367603	1177.014090	16.208947
26.434128	1190.814768	16.213965
26.402926	1178.876400	16.218983
26.501761	1196.661439	16.224000
26.267297	1217.473926	16.229018
26.508333	1217.211273	16.234035
26.402685	1226.223898	16.239053
26.460662	1219.806674	16.244071
26.597756	1218.530854	16.249088
26.634113	1226.056668	16.254106
26.567337	1228.474572	16.259123
26.755173	1222.072890	16.264141
26.932052	1220.791675	16.269159
26.968143	1219.153277	16.274176
26.521803	1221.345368	16.279194
26.806367	1214.130984	16.284211
26.959583	1216.174202	16.289229
27.189476	1218.443883	16.294247
26.998672	1214.880897	16.299264
26.524493	1217.475358	16.304282
27.115148	1215.609906	16.309299
26.959420	1223.323341	16.314317
27.154652	1233.781085	16.319335
27.273682	1241.697904	16.324352
27.007365	1243.798448	16.329370
26.928622	1238.515639	16.334387
26.948984	1249.864750	16.339405
27.109582	1243.594509	16.344423
27.063534	1239.799559	16.349440
27.411324	1254.786883	16.354458
27.406140	1242.336572	16.359475
27.197288	1243.156565	16.364493
27.461204	1248.412665	16.369511
27.505923	1250.284674	16.374528
27.434145	1248.799312	16.379546
27.451425	1248.555330	16.384563
27.377972	1234.936772	16.389581
27.220310	1241.115351	16.394599
27.457209	1233.089282	16.399616
27.432979	1242.480328	16.404634
27.677852	1247.566768	16.409651
27.680777	1241.008461	16.414669
27.506432	1234.511925	16.419687
27.462218	1229.532221	16.424704
27.296400	1236.268355	16.429722
27.786111	1242.245286	16.434739
27.837808	1233.545605	16.439757
27.585816	1248.064413	16.444775
27.727971	1246.138646	16.449792
27.645873	1262.521214	16.454810
27.936783	1270.889292	16.459827
27.983906	1270.713398	16.464845
27.748219	1271.052274	16.469863
28.194434	1271.496147	16.474880
28.030909	1271.886278	16.479898
28.107753	1255.701340	16.484915
28.258216	1263.512205	16.489933
27.790498	1257.906722	16.494951
28.223819	1261.304024	16.499968
27.796193	1272.130034	16.504986
27.868033	1265.758327	16.510003
28.152233	1273.450459	16.515021
27.999017	1269.702144	16.520039
28.274238	1273.456821	16.525056
28.054042	1273.285148	16.530074
28.112259	1265.232103	16.535091
28.361854	1274.328155	16.540109
27.996543	1264.088569	16.545127
28.427218	1256.187332	16.550144
28.309165	1269.961702	16.555162
28.003185	1266.138845	16.560179
28.575154	1264.210344	16.565197
28.411786	1269.465616	16.570215
28.654124	1266.595093	16.575232
28.252147	1270.449671	16.580250
28.420715	1269.326101	16.585267
28.103930	1266.566868	16.590285
28.013985	1281.763147	16.595303
28.187931	1284.610300	16.600320
28.310923	1292.266099	16.605338
28.584048	1289.630603	16.610355
28.670128	1290.067268	16.615373
28.653837	1291.255969	16.620391
29.070772	1293.014711	16.625408
28.977865	1290.692221	16.630426
29.056350	1298.171942	16.635443
28.949412	1300.207776	16.640461
28.989168	1283.767365	16.645479
29.476292	1286.656845	16.650496
29.127056	1296.386625	16.655514
29.008078	1287.641114	16.660531
28.997968	1294.453691	16.665549
29.033955	1289.785073	16.670567
28.776816	1285.629388	16.675584
29.098289	1291.384180	16.680602
29.012990	1292.842512	16.685619
29.397578	1292.585461	16.690637
29.211709	1286.962914	16.695655
29.352932	1278.160239	16.700672
29.249551	1282.458902	16.705690
29.005912	1286.550466	16.710707
29.521552	1284.822383	16.715725
28.944540	1285.029899	16.720743
28.858646	1290.898063	16.725760
28.671647	1284.757872	16.730778
28.975346	1291.608734	16.735795
29.346675	1290.393397	16.740813
29.202073	1318.239860	16.745831
29.794089	1307.310830	16.750848
29.761230	1317.337499	16.755866
29.541328	1319.268203	16.760883
29.918021	1312.796305	16.765901
29.600921	1303.813488	16.770919
29.702556	1286.423233	16.775936
29.821934	1276.912863	16.780954
29.628412	1279.059050	16.785971
29.550980	1287.414790	16.790989
29.423803	1293.642871	16.796007
29.846668	1304.917046	16.801024
29.862025	1313.007112	16.806042
29.869631	1321.998912	16.811059
29.781894	1314.076440	16.816077
29.917155	1319.728374	16.821095
30.052847	1319.305793	16.826112
30.231965	1321.654145	16.831130
30.130518	1314.092544	16.836147
30.124525	1299.358623	16.841165
29.873501	1298.372684	16.846183
30.191633	1298.986519	16.851200
29.894068	1299.631048	16.856218
29.978378	1303.708377	16.861235
29.919743	1310.372902	16.866253
29.998991	1314.145607	16.871271
30.071509	1311.533220	16.876288
30.059623	1306.365303	16.881306
30.241721	1311.853416	16.886323
30.270807	1316.363824	16.891341
30.111370	1317.572836	16.896359
30.252729	1311.435057	16.901376
30.304252	1314.161327	16.906394
30.255119	1312.808022	16.911411
30.156006	1307.130586	16.916429
30.033736	1308.474969	16.921447
30.203043	1333.980576	16.926464
30.193820	1344.552485	16.931482
30.150026	1344.995261	16.936499
30.677485	1336.208045	16.941517
30.674038	1342.492853	16.946535
30.668814	1339.031434	16.951552
30.492336	1344.691395	16.956570
30.329744	1340.795225	16.961587
30.522613	1338.255451	16.966605
30.590924	1343.610631	16.971623
30.473960	1346.164977	16.976640
30.784597	1351.439766	16.981658
31.004894	1378.143723	16.986675
31.371637	1366.661220	16.991693
30.964108	1360.738713	16.996711
31.060122	1339.429260	17.001728
30.880309	1342.806661	17.006746
30.884555	1333.926802	17.011763
31.178725	1324.606185	17.016781
31.105013	1341.357275	17.021799
30.914552	1331.527068	17.026816
30.980671	1351.048328	17.031834
30.837828	1359.324772	17.036851
31.579624	1359.702090	17.041869
31.301065	1363.438279	17.046887
31.192203	1362.645543	17.051904
31.273078	1370.013897	17.056922
31.046160	1371.728675	17.061939
31.278372	1366.666638	17.066957
31.518085	1375.117041	17.071975
31.423170	1372.646666	17.076992
31.723936	1366.409896	17.082010
31.371784	1363.647829	17.087027
31.542513	1367.545959	17.092045
31.764909	1363.963468	17.097063
31.627625	1363.497820	17.102080
31.915934	1366.886438	17.107098
31.559588	1365.057008	17.112115
31.745260	1363.218115	17.117133
31.922001	1357.370882	17.122151
31.797212	1352.325331	17.127168
31.973108	1360.515645	17.132186
31.594449	1364.746846	17.137203
31.791722	1358.725773	17.142221
32.188105	1366.759791	17.147239
31.879637	1367.970997	17.152256
31.865112	1354.683684	17.157274
31.645748	1360.579836	17.162291
31.920528	1363.098578	17.167309
32.145677	1363.318592	17.172327
31.846376	1366.587417	17.177344
31.829199	1356.679747	17.182362
31.609157	1359.775851	17.187379
32.019270	1357.211196	17.192397
31.895496	1364.979255	17.197415
32.159815	1356.240629	17.202432
32.213377	1357.792538	17.207450
32.273050	1365.394673	17.212467
32.367947	1355.344684	17.217485
32.103669	1355.620974	17.222503
32.091761	1373.767378	17.227520
32.053992	1382.941096	17.232538
31.975719	1388.741709	17.237555
32.459324	1387.726282	17.242573
32.380544	1389.192600	17.247591
32.132720	1393.877116	17.252608
32.436441	1384.441714	17.257626
31.935815	1389.449065	17.262643
32.226491	1394.356555	17.267661
32.230815	1407.363891	17.272679
32.559203	1412.219098	17.277696
32.569710	1405.972019	17.282714
32.471537	1412.901745	17.287731
33.278438	1409.686167	17.292749
33.165366	1415.907834	17.297767
32.883560	1411.803034	17.302784
33.174442	1405.873741	17.307802
33.092769	1402.155494	17.312819
33.023951	1407.025362	17.317837
33.229823	1402.647879	17.322855
32.922732	1398.582099	17.327872
32.729779	1393.800713	17.332890
32.797281	1400.382829	17.337907
33.313989	1389.081598	17.342925
33.120304	1402.311780	17.347943
33.307318	1402.269634	17.352960
33.406589	1396.756399	17.357978
33.075253	1408.694768	17.362995
33.286867	1397.532124	17.368013
33.635728	1401.669487	17.373031
33.435060	1405.385336	17.378048
33.649705	1400.156138	17.383066
33.341595	1411.983798	17.388083
33.480343	1410.124115	17.393101
33.559544	1403.128985	17.398119
33.380283	1400.563701	17.403136
33.317792	1399.991612	17.408154
33.280431	1409.184566	17.413171
33.432065	1402.471123	17.418189
33.562416	1407.912121	17.423207
33.107034	1417.398337	17.428224
33.742265	1405.755903	17.433242
33.445985	1416.244609	17.438259
33.161265	1409.856185	17.443277
33.751464	1410.311501	17.448295
34.027068	1420.518725	17.453312
34.087302	1423.443348	17.458330
33.664341	1419.524643	17.463347
34.024247	1430.847892	17.468365
34.050994	1428.378659	17.473383
34.001616	1433.453560	17.478400
34.279402	1430.467716	17.483418
34.072561	1419.298627	17.488435
34.120864	1408.089549	17.493453
34.002836	1406.829892	17.498471
33.664416	1428.542387	17.503488
34.263415	1421.727453	17.508506
34.149672	1428.965226	17.513523
33.962617	1429.277567	17.518541
34.582504	1417.926200	17.523559
34.328418	1428.585473	17.528576
34.581264	1421.608483	17.533594
34.133398	1427.037968	17.538611
34.243282	1424.901206	17.543629
34.765806	1422.653938	17.548647
34.212504	1428.370098	17.553664
34.495166	1418.952916	17.558682
34.583168	1430.197690	17.563699
34.522045	1421.173684	17.568717
34.527957	1431.137927	17.573735
34.085791	1422.191650	17.578752
34.236749	1419.693036	17.583770
34.359172	1436.190001	17.588787
34.632506	1446.647383	17.593805
34.723430	1452.508041	17.598823
34.516958	1463.740880	17.603840
35.053190	1457.629706	17.608858
34.723888	1452.767109	17.613875
34.783363	1455.885929	17.618893
34.976354	1443.281267	17.623911
34.785363	1457.211341	17.628928
35.148583	1439.915066	17.633946
34.902446	1448.098407	17.638963
34.741534	1446.752343	17.643981
35.083288	1449.542077	17.648999
34.789401	1447.789901	17.654016
35.020281	1447.624972	17.659034
35.467172	1458.237317	17.664051
35.391091	1462.947796	17.669069
35.683533	1472.523429	17.674087
35.389814	1455.204810	17.679104
35.290998	1444.927953	17.684122
35.394895	1448.035495	17.689139
35.528503	1456.518435	17.694157
35.097540	1458.977466	17.699175
35.205423	1469.759996	17.704192
35.295230	1466.149597	17.709210
35.540764	1471.210613	17.714227
35.496143	1468.439433	17.719245
35.499885	1456.813926	17.724263
35.502673	1469.279720	17.729280
35.416154	1459.187408	17.734298
35.572330	1463.455827	17.739315
35.710148	1463.325761	17.744333
35.580456	1472.083683	17.749351
35.774665	1493.833825	17.754368
36.329050	1485.897660	17.759386
36.090228	1492.723123	17.764403
36.128321	1486.778298	17.769421
36.431588	1475.329429	17.774439
35.996488	1474.484904	17.779456
36.136863	1461.712373	17.784474
35.996095	1463.649700	17.789491
36.276905	1476.657659	17.794509
36.632958	1478.359171	17.799527
36.065610	1474.251547	17.804544
35.934748	1463.093883	17.809562
35.907912	1469.893360	17.814579
36.229055	1479.677214	17.819597
36.437376	1478.771043	17.824615
36.337231	1485.974907	17.829632
36.381076	1479.926392	17.834650
36.581494	1485.413311	17.839667
36.426574	1488.222145	17.844685
36.513888	1483.606985	17.849703
36.321089	1484.804990	17.854720
36.737207	1490.061413	17.859738
36.687712	1493.558629	17.864755
36.578291	1490.259453	17.869773
36.762412	1494.924976	17.874791
36.257447	1497.079948	17.879808
36.276123	1490.255780	17.884826
36.383362	1494.679517	17.889843
36.645970	1514.855621	17.894861
36.543516	1516.627394	17.899879
36.854019	1526.268569	17.904896
37.023277	1506.411730	17.909914
37.305741	1508.943792	17.914931
37.001101	1527.783344	17.919949
37.260730	1507.187461	17.924967
37.137243	1521.370769	17.929984
37.043185	1514.885647	17.935002
37.743642	1511.282579	17.940019
37.262780	1525.231092	17.945037
37.307261	1499.243400	17.950055
37.304602	1515.495803	17.955072
37.298907	1501.585537	17.960090
37.414509	1509.763653	17.965107
37.135381	1516.898303	17.970125
37.550084	1509.792179	17.975143
37.256762	1516.744950	17.980160
37.310201	1503.336647	17.985178
37.445003	1507.939468	17.990195
37.211396	1508.454751	17.995213
37.487258	1515.886609	18.000231
37.380245	1532.060619	18.005248
37.868957	1541.829420	18.010266
38.023765	1539.562597	18.015283
37.918493	1545.601753	18.020301
38.237859	1538.150399	18.025319
37.577698	1529.544960	18.030336
38.024746	1525.737934	18.035354
38.195029	1528.728631	18.040371
37.814992	1535.185576	18.045389
37.910352	1534.646050	18.050407
38.062460	1543.965823	18.055424
37.820348	1541.259348	18.060442
38.191417	1529.782308	18.065459
38.211442	1541.487152	18.070477
38.464021	1529.341994	18.075495
38.182263	1530.890482	18.080512
37.903426	1539.017670	18.085530
38.251937	1530.304791	18.090547
38.028906	1533.771056	18.095565
38.263665	1535.069844	18.100583
38.258043	1540.184786	18.105600
38.089913	1537.809935	18.110618
38.287815	1542.329318	18.115635
38.305654	1560.853847	18.120653
38.832785	1556.429925	18.125671
38.658272	1559.418755	18.130688
38.514790	1561.796836	18.135706
38.799171	1560.472242	18.140723
38.777278	1563.926926	18.145741
38.578791	1547.905864	18.150759
38.525276	1558.130368	18.155776
38.221377	1555.112689	18.160794
38.476237	1555.298864	18.165811
38.516418	1560.064757	18.170829
38.649728	1568.365551	18.175847
38.972364	1580.838611	18.180864
38.932496	1581.389391	18.185882
39.213104	1581.156606	18.190899
39.073558	1584.108762	18.195917
39.198455	1566.246695	18.200935
39.125115	1580.036195	18.205952
39.147350	1584.883593	18.210970
39.246784	1574.186542	18.215987
39.055433	1577.490319	18.221005
39.050753	1565.710435	18.226023
38.918106	1573.678266	18.231040
39.053202	1582.461972	18.236058
39.818718	1590.330596	18.241075
39.557358	1590.791224	18.246093
39.910631	1597.193148	18.251111
39.898696	1582.689630	18.256128
39.752588	1571.504686	18.261146
39.949230	1567.888811	18.266163
39.612891	1570.643005	18.271181
39.625577	1563.167918	18.276199
39.626460	1569.270830	18.281216
39.788605	1558.919871	18.286234
40.172875	1561.255223	18.291251
39.567438	1572.420428	18.296269
39.878120	1565.853048	18.301287
40.125156	1587.943364	18.306304
40.096986	1581.454805	18.311322
39.983037	1573.211182	18.316339
40.156467	1588.659673	18.321357
40.095433	1586.673753	18.326375
40.082254	1585.218040	18.331392
40.052755	1600.675671	18.336410
40.233498	1592.445930	18.341427
40.229414	1593.955231	18.346445
40.223835	1593.742183	18.351463
40.135763	1596.523653	18.356480
40.165108	1594.425960	18.361498
40.368338	1594.704317	18.366515
40.117922	1596.282667	18.371533
40.277235	1593.571847	18.376551
39.996385	1594.059314	18.381568
40.184887	1617.926621	18.386586
40.472019	1624.397352	18.391603
40.285821	1620.371566	18.396621
40.572027	1622.344640	18.401639
40.888185	1620.400111	18.406656
40.880944	1624.618818	18.411674
40.970796	1611.057574	18.416691
40.934527	1621.783334	18.421709
41.097178	1617.364711	18.426727
41.018523	1618.155728	18.431744
40.870213	1616.206074	18.436762
41.115849	1613.150519	18.441779
41.442899	1616.711506	18.446797
41.346327	1616.264316	18.451815
41.062998	1610.140109	18.456832
41.023902	1618.929003	18.461850
40.973767	1616.535625	18.466867
41.439187	1615.684782	18.471885
41.366147	1627.423965	18.476903
41.574901	1616.303559	18.481920
41.108025	1620.368526	18.486938
41.120806	1630.451038	18.491955
41.252551	1642.081796	18.496973
41.283715	1651.580457	18.501991
41.505128	1650.463676	18.507008
41.412145	1651.117711	18.512026
41.944970	1643.502309	18.517043
41.505929	1652.435255	18.522061
41.227335	1647.907280	18.527079
41.607920	1639.883631	18.532096
41.681025	1659.353151	18.537114
41.887752	1662.307541	18.542131
42.051929	1669.453443	18.547149
42.176162	1668.546001	18.552167
42.410799	1665.574920	18.557184
42.397886	1649.681725	18.562202
42.576648	1629.466512	18.567219
42.457710	1634.361661	18.572237
42.154172	1631.742672	18.577255
42.498626	1634.772119	18.582272
42.392509	1631.562314	18.587290
42.274614	1631.368613	18.592307
42.607170	1626.271015	18.597325
42.422760	1636.117255	18.602343
42.556947	1623.318845	18.607360
42.180205	1634.017818	18.612378
42.426428	1629.438550	18.617395
42.403975	1633.264158	18.622413
42.371969	1629.874807	18.627431
42.762504	1621.930024	18.632448
42.193201	1629.523054	18.637466
42.346723	1623.469744	18.642483
42.485690	1643.616455	18.647501
42.403275	1650.901510	18.652519
42.838425	1665.778161	18.657536
42.926837	1675.132158	18.662554
42.846401	1669.212951	18.667571
42.377174	1672.049547	18.672589
42.293779	1664.713303	18.677607
43.023425	1659.975609	18.682624
42.851664	1671.705552	18.687642
43.176058	1684.876345	18.692659
42.997328	1698.713874	18.697677
42.988536	1697.309583	18.702695
42.919621	1697.216434	18.707712
42.871897	1702.651535	18.712730
42.717190	1695.241836	18.717747
42.898706	1695.731237	18.722765
43.398544	1718.967605	18.727783
43.680603	1716.388822	18.732800
43.517035	1719.053869	18.737818
43.730506	1720.087525	18.742835
43.799591	1715.985477	18.747853
43.809328	1726.375799	18.752871
44.114614	1716.673041	18.757888
43.709377	1700.372640	18.762906
43.696276	1690.824466	18.767923
43.635459	1700.310015	18.772941
43.866385	1706.631232	18.777959
44.329186	1714.544039	18.782976
43.973846	1715.935042	18.787994
44.051165	1723.119728	18.793011
44.088022	1716.499319	18.798029
44.314584	1708.063939	18.803047
44.549551	1708.583676	18.808064
44.044680	1692.859714	18.813082
44.052391	1704.244711	18.818099
44.286723	1706.363752	18.823117
44.385425	1706.347222	18.828135
44.739219	1715.485168	18.833152
44.565545	1708.900733	18.838170
44.223278	1692.077601	18.843187
44.314601	1701.168372	18.848205
44.042359	1710.292263	18.853223
44.388265	1698.367937	18.858240
44.228649	1706.526095	18.863258
44.555819	1717.250321	18.868275
44.897311	1716.162899	18.873293
44.733818	1719.349717	18.878311
44.748083	1698.160940	18.883328
44.686558	1710.312795	18.888346
44.617649	1709.890358	18.893363
44.740652	1717.388907	18.898381
44.508952	1728.076770	18.903399
44.761132	1739.514100	18.908416
44.602277	1745.402367	18.913434
44.695387	1739.187560	18.918451
44.930566	1744.649342	18.923469
44.883192	1738.231401	18.928487
44.961588	1736.608001	18.933504
45.244273	1755.093132	18.938522
45.297821	1760.659728	18.943539
45.456652	1762.513337	18.948557
45.462542	1760.073478	18.953575
45.896222	1761.402989	18.958592
45.856571	1752.052644	18.963610
45.784906	1739.380662	18.968627
45.754845	1723.634104	18.973645
45.364598	1729.269105	18.978663
45.519501	1713.951381	18.983680
45.447741	1729.012240	18.988698
45.588754	1745.105139	18.993715
45.768327	1754.444514	18.998733
45.825976	1758.741697	19.003751
46.121521	1756.627154	19.008768
45.850066	1767.264731	19.013786
46.027977	1756.158769	19.018803
46.124875	1761.110209	19.023821
45.754449	1763.503384	19.028839
45.985233	1751.705310	19.033856
45.883961	1751.358092	19.038874
45.986876	1753.572273	19.043891
46.221252	1750.365815	19.048909
45.915226	1749.752668	19.053927
46.072416	1757.922076	19.058944
45.963160	1782.748765	19.063962
46.197978	1791.949129	19.068979
46.698209	1776.012735	19.073997
46.346600	1785.297601	19.079015
46.699014	1775.002447	19.084032
46.701054	1785.413172	19.089050
46.809682	1782.161158	19.094067
46.824582	1772.608306	19.099085
46.544772	1772.141200	19.104103
46.587697	1772.114992	19.109120
46.835538	1782.157972	19.114138
46.412322	1777.300358	19.119155
46.827090	1774.594925	19.124173
47.049600	1788.572503	19.129191
47.423063	1794.708806	19.134208
47.549406	1805.123213	19.139226
47.390923	1788.914012	19.144243
47.261223	1779.968639	19.149261
47.251686	1781.606008	19.154279
47.287653	1773.942546	19.159296
47.312537	1779.402679	19.164314
47.440965	1771.189952	19.169331
47.514636	1778.163877	19.174349
47.178353	1780.330967	19.179367
47.668323	1791.109829	19.184384
47.690664	1784.635472	19.189402
47.409846	1795.420857	19.194419
47.647416	1788.814290	19.199437
47.715526	1804.850804	19.204455
47.963994	1787.314474	19.209472
47.699083	1795.847121	19.214490
47.612997	1794.177676	19.219507
47.874924	1789.738072	19.224525
47.589216	1797.248694	19.229543
47.672535	1790.561134	19.234560
47.623543	1804.294652	19.239578
47.657382	1806.712947	19.244595
47.709486	1809.683863	19.249613
48.015946	1821.975564	19.254631
48.289442	1822.813898	19.259648
48.399095	1817.850698	19.264666
47.935241	1829.746731	19.269683
48.132176	1815.176199	19.274701
48.122432	1824.782108	19.279719
48.070884	1815.118179	19.284736
48.265053	1832.328820	19.289754
48.326049	1839.529446	19.294771
48.509460	1846.726773	19.299789
48.460725	1851.777298	19.304807
48.951735	1844.399980	19.309824
48.983023	1838.083748	19.314842
48.681802	1842.463679	19.319859
48.901979	1827.605077	19.324877
48.983118	1852.768482	19.329895
49.129695	1838.906951	19.334912
49.172376	1837.974398	19.339930
48.949056	1835.796786	19.344947
49.103437	1834.830619	19.349965
48.892502	1836.374125	19.354983
48.993283	1837.676774	19.360000
49.019901	1838.118557	19.365018
49.060030	1849.028678	19.370035
49.558992	1837.258852	19.375053
49.339355	1837.952523	19.380071
49.016977	1848.710171	19.385088
49.579310	1846.179923	19.390106
49.663579	1871.386930	19.395123
49.588504	1866.110778	19.400141
49.503786	1871.138716	19.405159
49.511614	1873.735905	19.410176
49.540918	1866.599812	19.415194
49.560664	1870.914902	19.420211
49.904984	1862.209616	19.425229
50.048595	1870.386052	19.430247
49.726448	1870.743753	19.435264
49.677561	1857.046183	19.440282
49.535907	1875.300633	19.445299
50.343212	1865.377636	19.450317
49.945731	1871.113084	19.455335
50.419448	1884.998261	19.460352
50.695190	1875.262889	19.465370
50.190628	1880.411777	19.470387
50.148017	1866.296085	19.475405
50.141087	1886.309763	19.480423
50.579262	1885.472463	19.485440
50.990057	1899.168861	19.490458
50.845776	1883.284143	19.495475
50.406141	1861.664893	19.500493
50.409090	1877.077680	19.505511
50.433357	1883.952153	19.510528
50.657141	1884.843188	19.515546
50.418236	1894.952505	19.520563
50.740915	1885.866379	19.525581
50.452752	1891.346790	19.530599
50.669733	1890.424402	19.535616
50.909613	1888.297587	19.540634
50.824308	1890.706059	19.545651
50.871464	1906.280645	19.550669
51.021673	1906.692953	19.555687
51.329908	1908.012109	19.560704
51.205671	1904.817641	19.565722
50.994024	1916.365997	19.570739
51.304273	1918.779771	19.575757
51.511438	1913.274307	19.580775
51.015699	1916.215119	19.585792
51.885950	1905.981140	19.590810
51.702428	1917.816351	19.595827
51.703839	1909.084249	19.600845
51.589860	1912.995121	19.605863
51.668508	1907.805153	19.610880
51.740867	1904.808880	19.615898
51.405217	1913.819367	19.620915
51.666781	1899.094785	19.625933
51.849102	1907.630746	19.630951
51.655581	1910.374192	19.635968
51.833200	1912.477047	19.640986
51.797269	1922.846901	19.646003
52.052870	1942.514548	19.651021
52.168105	1940.581137	19.656039
52.209331	1943.608989	19.661056
52.501666	1939.677644	19.666074
52.129944	1941.938988	19.671091
52.421653	1933.851734	19.676109
52.424351	1935.610903	19.681127
52.283466	1926.062442	19.686144
52.685506	1925.439355	19.691162
52.392038	1933.690806	19.696179
52.358072	1934.065053	19.701197
52.311115	1929.564063	19.706215
52.369957	1928.548134	19.711232
52.358564	1935.070100	19.716250
52.661954	1960.479205	19.721267
52.856138	1964.438368	19.726285
52.864185	1952.669863	19.731303
52.956754	1960.517812	19.736320
52.917494	1956.633581	19.741338
52.765386	1957.868987	19.746355
53.136061	1951.185048	19.751373
52.771877	1943.141220	19.756391
53.343546	1955.830688	19.761408
53.227386	1956.822582	19.766426
53.039499	1963.307197	19.771443
53.557323	1978.159271	19.776461
53.314068	1987.676127	19.781479
53.444775	1987.498814	19.786496
53.724412	1986.382624	19.791514
53.766481	1983.988320	19.796531
53.983668	1974.786518	19.801549
53.917390	1988.393741	19.806567
53.934012	1986.279398	19.811584
54.068438	1982.542621	19.816602
54.022473	1979.247812	19.821619
53.930677	1983.993130	19.826637
54.101176	1973.762941	19.831655
54.047129	1985.584682	19.836672
53.973757	1977.724840	19.841690
53.782347	1981.731193	19.846707
53.894054	1976.053510	19.851725
54.071140	1981.361413	19.856743
53.914407	1980.033112	19.861760
54.248795	1976.342222	19.866778
54.211702	1990.704773	19.871795
54.170697	1998.076052	19.876813
54.049624	1998.218856	19.881831
53.836413	2010.376725	19.886848
54.150326	2010.755095	19.891866
54.149974	2019.526792	19.896883
54.648549	2037.075113	19.901901
54.818696	2039.500051	19.906919
54.592047	2042.672767	19.911936
54.927595	2035.949719	19.916954
55.076178	2034.367243	19.921971
55.073994	2034.590982	19.926989
55.521386	2018.691807	19.932007
55.022377	2028.641065	19.937024
55.411058	2028.335108	19.942042
54.961443	2033.300576	19.947059
55.173644	2029.262975	19.952077
55.317654	2030.462248	19.957095
55.437152	2035.628718	19.962112
55.584235	2023.401011	19.967130
55.346730	2029.145313	19.972147
55.010288	2023.715468	19.977165
55.341048	2030.149441	19.982183
55.577138	2045.099902	19.987200
55.747521	2050.038898	19.992218
55.666447	2056.081144	19.997235
55.863566	2055.758618	20.002253
55.771661	2052.693014	20.007271
55.747070	2053.534759	20.012288
55.970425	2050.460952	20.017306
55.882802	2051.433572	20.022323
55.867721	2048.392474	20.027341
55.872848	2055.561296	20.032359
55.914206	2062.697366	20.037376
56.200558	2063.693021	20.042394
56.307895	2089.838795	20.047411
56.089976	2089.988747	20.052429
56.409785	2079.207296	20.057447
56.443224	2081.436350	20.062464
56.371856	2069.422835	20.067482
56.402086	2082.734696	20.072499
55.988060	2074.919878	20.077517
56.474435	2087.357042	20.082535
56.926784	2100.632822	20.087552
57.005512	2104.417026	20.092570
57.256702	2100.797919	20.097587
57.099086	2104.472769	20.102605
57.550664	2095.156975	20.107623
57.163153	2078.902252	20.112640
57.224938	2079.011691	20.117658
57.234922	2066.540688	20.122675
56.837006	2068.285962	20.127693
56.843033	2073.931186	20.132711
57.097657	2095.410414	20.137728
57.348144	2082.810098	20.142746
57.243036	2094.484471	20.147763
56.995995	2106.220885	20.152781
57.265438	2092.968481	20.157799
57.127394	2123.286706	20.162816
57.501462	2116.260635	20.167834
57.625792	2124.156170	20.172851
57.685498	2120.718291	20.177869
57.690093	2121.357205	20.182887
57.664157	2140.982269	20.187904
57.679340	2122.708008	20.192922
57.822206	2139.040161	20.197939
57.957450	2149.219693	20.202957
58.447084	2151.305269	20.207975
58.469510	2162.724982	20.212992
58.595100	2151.328003	20.218010
58.625029	2149.307492	20.223027
58.777883	2140.461463	20.228045
59.159152	2130.185713	20.233063
58.526945	2121.681999	20.238080
58.599320	2119.782221	20.243098
58.592856	2103.205281	20.248115
58.430954	2113.532110	20.253133
58.825901	2109.803034	20.258151
58.485087	2123.747050	20.263168
58.466678	2127.820708	20.268186
58.605814	2141.352984	20.273203
58.605363	2151.551004	20.278221
58.950790	2137.686854	20.283239
58.884709	2139.192085	20.288256
58.749162	2139.249496	20.293274
59.004551	2150.324632	20.298291
59.020922	2155.450513	20.303309
59.484508	2167.980279	20.308327
59.641632	2166.061373	20.313344
59.660179	2169.006215	20.318362
59.648023	2165.199728	20.323379
59.398141	2167.361254	20.328397
59.602900	2162.965633	20.333415
59.703323	2156.208362	20.338432
59.599172	2168.665034	20.343450
59.719510	2173.679065	20.348467
59.563112	2164.020826	20.353485
60.222108	2170.110097	20.358503
59.774079	2163.402119	20.363520
59.901272	2160.901605	20.368538
60.307620	2169.250313	20.373555
59.947784	2175.168215	20.378573
60.069872	2153.927533	20.383591
59.746380	2168.894803	20.388608
60.099750	2167.560335	20.393626
60.471350	2183.900797	20.398643
60.351208	2189.961754	20.403661
60.502114	2189.811413	20.408679
60.494117	2194.377807	20.413696
60.721327	2193.286997	20.418714
60.492883	2179.550314	20.423731
60.522837	2197.429183	20.428749
60.539875	2187.667868	20.433767
60.630720	2188.725561	20.438784
60.574041	2188.902603	20.443802
60.816198	2197.541818	20.448819
60.834193	2221.738011	20.453837
61.133591	2211.592456	20.458855
60.912668	2218.516255	20.463872
61.006357	2223.080420	20.468890
61.593554	2213.881895	20.473907
61.222963	2224.766853	20.478925
61.294794	2214.283347	20.483943
61.261488	2220.990927	20.488960
61.354065	2220.702010	20.493978
61.839729	2224.351289	20.498995
61.411845	2228.421582	20.504013
61.769186	2235.591139	20.509031
61.638834	2244.840307	20.514048
62.164875	2252.863800	20.519066
62.337999	2233.565963	20.524083
62.011735	2237.574588	20.529101
62.062299	2233.157187	20.534119
62.394561	2244.672794	20.539136
62.481168	2235.566818	20.544154
62.326665	2236.430237	20.549171
62.235174	2230.499452	20.554189
62.257251	2232.561328	20.559207
62.339378	2226.892968	20.564224
62.236319	2232.269690	20.569242
62.578487	2221.281119	20.574259
62.449989	2238.884872	20.579277
62.310005	2231.785442	20.584295
62.766721	2230.175845	20.589312
62.607839	2236.080247	20.594330
62.812514	2224.799463	20.599347
62.751044	2233.191656	20.604365
63.085901	2239.661652	20.609383
62.990896	2251.493710	20.614400
62.776809	2265.124223	20.619418
63.156116	2252.889453	20.624435
62.765090	2262.196274	20.629453
62.912365	2269.941452	20.634471
63.167266	2263.583765	20.639488
63.127128	2266.928246	20.644506
63.215083	2258.331040	20.649523
62.969702	2270.890061	20.654541
63.569919	2272.116123	20.659559
63.568991	2275.223243	20.664576
63.437450	2271.758081	20.669594
63.742918	2277.622573	20.674611
63.290527	2285.803237	20.679629
63.515286	2272.482677	20.684647
63.802074	2271.402684	20.689664
63.503419	2279.349299	20.694682
64.054898	2294.933451	20.699699
63.960920	2306.485290	20.704717
64.221862	2317.772405	20.709735
64.669393	2309.513551	20.714752
64.575586	2312.672047	20.719770
64.552378	2301.847330	20.724787
64.499722	2309.642690	20.729805
64.445217	2304.609028	20.734823
64.647844	2300.900862	20.739840
64.819608	2300.731720	20.744858
64.561810	2297.649783	20.749875
64.494386	2294.646418	20.754893
64.533585	2295.328829	20.759911
64.911311	2295.545890	20.764928
64.518837	2306.082586	20.769946
64.974943	2317.208722	20.774963
65.102469	2322.025569	20.779981
65.259621	2324.856600	20.784999
65.103400	2330.393899	20.790016
64.837054	2335.478573	20.795034
65.069776	2323.014647	20.800051
65.036932	2327.587351	20.805069
65.438849	2345.699389	20.810087
65.823862	2350.508930	20.815104
66.121022	2366.415273	20.820122
66.111753	2338.297246	20.825139
65.989459	2333.419842	20.830157
65.770278	2327.806550	20.835175
65.972602	2326.313777	20.840192
65.829753	2321.637787	20.845210
65.803608	2326.746344	20.850227
65.863034	2353.241789	20.855245
66.074386	2346.684590	20.860263
66.128290	2351.402992	20.865280
66.269132	2355.663171	20.870298
66.035546	2346.675388	20.875315
66.270093	2355.533843	20.880333
66.131280	2351.439999	20.885351
66.327933	2362.687382	20.890368
66.400146	2374.116541	20.895386
66.706410	2378.623383	20.900403
66.483314	2378.622434	20.905421
66.425680	2380.880753	20.910439
66.808802	2379.467342	20.915456
66.439096	2388.835079	20.920474
66.625346	2401.013064	20.925491
66.772626	2409.234058	20.930509
66.723660	2410.321562	20.935527
67.163996	2397.823268	20.940544
66.883318	2403.085121	20.945562
67.205155	2410.155517	20.950579
67.406442	2433.362977	20.955597
67.602947	2427.931331	20.960615
67.746850	2426.278926	20.965632
67.770177	2432.668997	20.970650
68.052273	2427.065544	20.975667
68.029566	2406.707226	20.980685
67.771225	2400.453780	20.985703
67.777623	2397.084880	20.990720
67.768923	2412.285776	20.995738
67.952432	2410.435112	21.000755
67.953950	2415.895592	21.005773
68.070741	2428.208491	21.010791
68.433596	2426.725794	21.015808
68.112817	2429.741913	21.020826
68.297653	2424.287002	21.025843
68.186702	2424.867666	21.030861
68.089179	2423.286256	21.035879
68.220442	2416.223211	21.040896
67.895414	2427.273602	21.045914
68.383794	2439.916807	21.050931
68.515303	2446.995444	21.055949
68.482171	2450.089419	21.060967
68.728719	2447.307937	21.065984
68.879980	2454.446695	21.071002
68.897285	2473.629442	21.076019
69.361772	2481.007374	21.081037
69.336724	2473.926238	21.086055
69.634727	2478.357709	21.091072
69.246497	2475.270520	21.096090
69.554263	2472.405303	21.101107
69.581881	2468.147520	21.106125
69.450886	2478.042944	21.111143
69.531488	2471.979504	21.116160
69.794446	2479.268502	21.121178
69.666711	2462.053986	21.126195
69.576974	2470.206116	21.131213
69.952893	2471.582637	21.136231
69.959588	2459.788379	21.141248
69.803065	2473.114312	21.146266
69.682547	2466.496163	21.151283
69.891387	2471.567118	21.156301
69.792075	2491.197272	21.161319
70.306812	2495.014831	21.166336
69.859915	2502.181199	21.171354
70.242822	2499.510433	21.176371
70.359487	2500.532190	21.181389
70.302456	2498.048286	21.186407
70.524438	2522.763167	21.191424
70.735202	2526.675449	21.196442
70.845439	2536.478887	21.201459
71.182642	2526.021983	21.206477
70.710324	2534.378497	21.211495
71.288321	2520.029350	21.216512
71.098363	2529.622764	21.221530
71.369611	2524.194677	21.226547
71.187339	2527.246191	21.231565
70.919348	2525.077632	21.236583
71.266512	2517.232663	21.241600
71.184173	2518.162710	21.246618
71.529546	2514.944447	21.251635
71.380119	2515.921009	21.256653
71.247710	2524.448104	21.261671
71.590847	2532.912959	21.266688
71.632741	2543.710099	21.271706
71.743586	2555.784732	21.276723
71.975422	2539.734634	21.281741
71.685401	2555.630729	21.286759
71.893606	2554.650114	21.291776
71.835130	2548.292130	21.296794
71.833459	2545.346349	21.301811
71.989608	2562.467837	21.306829
71.967083	2570.066041	21.311847
72.721696	2572.992668	21.316864
72.390138	2578.451556	21.321882
72.734926	2574.050985	21.326899
72.769366	2578.439037	21.331917
72.865665	2573.954537	21.336935
72.892948	2570.682338	21.341952
72.825345	2564.117800	21.346970
72.774874	2573.065207	21.351987
73.031939	2568.554931	21.357005
72.751179	2576.478269	21.362023
73.063582	2565.482170	21.367040
73.239930	2568.588990	21.372058
73.059299	2569.150271	21.377075
73.496631	2560.749477	21.382093
72.939504	2573.820852	21.387111
73.369459	2586.006347	21.392128
73.188164	2588.850443	21.397146
73.381940	2583.415454	21.402163
73.488171	2595.784362	21.407181
73.553500	2592.448198	21.412199
73.819627	2597.975049	21.417216
73.862021	2615.830695	21.422234
74.041142	2616.652193	21.427251
73.854557	2621.129335	21.432269
73.728234	2622.665431	21.437287
74.062623	2620.308742	21.442304
74.246709	2620.943803	21.447322
74.272567	2626.690079	21.452339
74.290821	2610.780902	21.457357
74.352268	2632.945903	21.462375
74.491306	2635.483746	21.467392
74.719066	2637.417994	21.472410
74.823036	2644.280422	21.477427
75.075548	2641.409739	21.482445
74.953809	2644.453635	21.487463
74.994277	2645.289975	21.492480
75.169292	2648.665320	21.497498
74.959565	2645.457070	21.502515
75.043125	2640.020196	21.507533
74.932367	2645.245982	21.512551
75.114639	2647.196802	21.517568
75.280502	2648.329132	21.522586
75.427040	2654.019258	21.527603
75.684126	2658.256180	21.532621
75.721291	2656.282238	21.537639
75.861134	2654.091541	21.542656
75.869178	2662.903946	21.547674
75.755967	2656.374266	21.552691
76.197659	2656.371330	21.557709
75.804103	2654.950616	21.562727
75.647054	2662.524445	21.567744
75.685724	2660.342592	21.572762
75.516895	2682.575634	21.577779
75.935482	2677.383957	21.582797
75.892257	2685.719643	21.587815
76.056522	2692.305022	21.592832
76.508217	2707.292344	21.597850
76.232497	2716.184541	21.602867
76.593208	2705.854332	21.607885
76.525233	2723.616341	21.612903
76.810309	2706.820313	21.617920
77.007535	2714.667296	21.622938
76.614394	2720.590317	21.627955
76.859380	2731.359540	21.632973
76.823097	2743.373400	21.637991
77.017427	2752.417852	21.643008
77.091926	2750.022992	21.648026
77.108460	2755.064799	21.653043
77.155005	2744.141637	21.658061
77.390336	2753.751325	21.663079
77.423149	2772.407307	21.668096
77.599507	2766.574960	21.673114
77.706881	2777.215586	21.678131
77.945889	2758.604393	21.683149
78.110587	2772.671942	21.688167
78.261041	2755.365070	21.693184
78.533623	2755.111356	21.698202
78.188034	2757.568287	21.703219
78.648658	2744.042216	21.708237
78.597169	2762.665269	21.713255
78.653916	2756.862533	21.718272
78.763438	2758.666738	21.723290
78.753560	2753.639924	21.728307
78.675457	2766.329568	21.733325
78.799346	2755.777845	21.738343
78.830904	2758.152772	21.743360
78.933490	2760.098665	21.748378
78.688649	2754.737079	21.753395
78.762720	2747.090261	21.758413
78.564744	2750.794766	21.763431
78.435551	2758.429388	21.768448
78.814080	2769.279124	21.773466
78.880405	2786.927680	21.778483
79.170570	2777.899158	21.783501
79.307927	2784.744913	21.788519
79.277923	2787.722500	21.793536
79.167935	2800.072186	21.798554
79.271677	2816.535923	21.803571
79.516374	2824.878435	21.808589
79.505554	2814.740642	21.813607
79.779757	2836.916445	21.818624
80.164340	2840.034577	21.823642
79.858180	2840.486696	21.828659
80.324744	2841.097332	21.833677
80.159525	2845.571992	21.838695
80.177800	2849.570688	21.843712
80.340225	2837.416570	21.848730
80.471878	2840.623346	21.853747
80.609776	2838.675450	21.858765
80.611642	2848.554471	21.863783
80.899369	2853.432606	21.868800
81.127745	2869.919505	21.873818
81.108145	2862.236143	21.878835
81.331858	2853.727192	21.883853
81.272182	2859.391433	21.888871
81.141021	2862.666443	21.893888
81.576370	2857.619959	21.898906
81.060599	2858.875176	21.903923
81.216425	2856.242464	21.908941
81.543551	2859.966912	21.913959
81.655517	2852.648014	21.918976
81.497413	2858.303324	21.923994
81.312587	2865.208257	21.929011
81.429220	2865.652715	21.934029
81.525120	2885.706991	21.939047
81.694549	2885.274269	21.944064
81.941027	2897.782834	21.949082
81.769001	2887.205514	21.954099
82.193837	2893.145985	21.959117
81.983564	2903.193947	21.964135
82.190344	2917.630638	21.969152
82.394429	2915.572982	21.974170
82.101083	2916.543824	21.979187
82.259481	2911.930075	21.984205
82.623538	2929.407554	21.989223
82.543848	2948.966152	21.994240
82.999887	2944.160697	21.999258
82.884139	2950.717657	22.004275
83.338984	2941.661435	22.009293
83.303424	2943.006983	22.014311
83.107839	2939.411118	22.019328
83.559275	2930.575533	22.024346
83.239985	2940.065972	22.029363
83.260769	2940.263292	22.034381
83.417597	2942.973827	22.039399
83.116003	2943.198434	22.044416
83.495760	2933.063736	22.049434
83.550531	2958.012840	22.054451
83.961741	2954.298200	22.059469
83.815535	2970.634515	22.064487
84.052089	2972.185088	22.069504
84.211868	2955.272495	22.074522
84.292893	2961.337912	22.079539
84.619754	2958.774948	22.084557
84.612508	2965.552162	22.089575
84.770110	2958.957920	22.094592
84.999622	2955.705172	22.099610
84.916995	2955.626287	22.104627
84.835234	2952.479697	22.109645
85.054124	2961.493443	22.114663
84.743489	2948.772558	22.119680
84.951754	2944.694232	22.124698
84.900727	2953.842334	22.129715
85.288432	2961.339677	22.134733
85.047701	2951.811016	22.139751
84.661674	2954.902187	22.144768
85.130378	2966.964659	22.149786
85.169484	2987.097346	22.154803
85.394263	2973.470684	22.159821
85.440924	2974.499120	22.164839
85.201585	2980.087193	22.169856
85.676421	2995.623308	22.174874
85.672805	3001.526358	22.179891
85.722286	3012.160178	22.184909
85.881222	3008.650590	22.189927
85.891943	3017.394844	22.194944
86.176296	3016.712430	22.199962
86.109149	3034.650634	22.204979
86.104302	3033.485717	22.209997
86.369223	3033.534433	22.215015
86.249404	3043.226608	22.220032
86.677525	3048.991802	22.225050
86.711361	3044.887157	22.230067
86.544481	3053.305677	22.235085
86.924923	3055.702129	22.240103
87.167463	3061.907425	22.245120
87.268026	3056.398504	22.250138
87.070734	3052.032062	22.255155
87.242799	3054.952690	22.260173
87.492160	3053.374521	22.265191
87.217747	3056.910634	22.270208
87.382249	3043.534018	22.275226
87.233436	3060.306272	22.280243
87.745072	3073.212877	22.285261
87.974360	3077.006298	22.290279
88.175970	3087.165051	22.295296
88.242941	3073.533277	22.300314
88.192732	3085.745365	22.305331
88.175186	3067.133284	22.310349
88.156791	3072.617954	22.315367
87.790380	3084.419319	22.320384
88.505834	3064.476721	22.325402
88.216943	3074.951546	22.330419
88.419810	3079.377260	22.335437
88.497965	3092.666521	22.340455
88.499817	3107.831712	22.345472
88.635885	3100.529973	22.350490
88.604532	3094.064137	22.355507
88.303755	3109.306895	22.360525
88.883308	3119.808318	22.365543
88.907870	3125.450076	22.370560
89.028858	3135.254087	22.375578
89.098542	3126.764926	22.380595
89.204205	3135.383721	22.385613
89.678070	3136.616762	22.390631
89.387278	3156.347900	22.395648
89.707494	3154.136777	22.400666
89.893749	3153.427262	22.405683
89.630357	3158.443017	22.410701
89.848906	3156.018780	22.415719
89.686291	3151.749332	22.420736
90.214394	3157.423640	22.425754
90.226772	3173.548931	22.430771
90.174138	3173.323755	22.435789
90.129449	3181.320199	22.440807
90.081885	3188.089212	22.445824
90.447110	3194.572309	22.450842
90.589140	3190.523761	22.455859
90.349279	3195.936019	22.460877
90.980077	3206.490844	22.465895
90.624853	3215.051986	22.470912
90.790085	3214.451844	22.475930
90.641936	3207.564330	22.480947
91.096622	3226.535781	22.485965
91.784826	3227.005484	22.490983
91.570561	3236.064588	22.496000
91.957087	3238.834069	22.501018
91.884444	3232.873013	22.506035
91.835298	3233.903519	22.511053
91.862684	3233.350956	22.516071
91.942656	3233.521570	22.521088
92.036403	3228.773139	22.526106
91.796288	3227.069543	22.531123
91.886227	3229.206950	22.536141
91.776746	3233.598891	22.541159
91.964794	3251.870362	22.546176
92.246734	3252.626482	22.551194
92.337371	3263.117457	22.556211
92.365683	3259.249488	22.561229
92.665852	3272.426235	22.566247
92.473831	3285.587476	22.571264
92.933061	3284.281684	22.576282
92.966093	3284.747448	22.581299
92.899250	3296.160505	22.586317
93.268616	3281.543174	22.591335
93.158160	3286.453386	22.596352
92.964841	3288.819097	22.601370
93.353612	3297.123886	22.606387
93.698455	3314.241995	22.611405
93.987888	3301.733859	22.616423
93.570940	3317.027117	22.621440
93.473749	3305.826925	22.626458
94.033579	3317.207310	22.631475
93.799939	3317.334080	22.636493
94.146740	3319.841249	22.641511
94.008734	3339.214704	22.646528
94.108164	3334.151530	22.651546
94.512096	3340.866477	22.656563
94.222376	3339.020674	22.661581
94.786359	3330.872942	22.666599
94.658519	3340.585525	22.671616
94.465699	3338.203646	22.676634
94.927457	3345.520441	22.681651
94.949124	3353.315462	22.686669
95.430548	3359.551088	22.691687
95.435429	3366.617804	22.696704
95.592292	3367.857579	22.701722
95.693992	3345.479092	22.706739
95.357707	3345.429915	22.711757
95.799586	3340.435740	22.716775
95.672607	3360.806981	22.721792
95.292413	3364.115372	22.726810
95.610390	3352.712689	22.731827
95.414770	3362.069172	22.736845
95.887057	3353.436592	22.741863
95.476336	3371.092202	22.746880
95.545455	3365.375380	22.751898
96.002028	3388.210013	22.756915
96.013826	3395.644095	22.761933
96.314455	3396.807362	22.766951
96.030164	3412.256348	22.771968
96.322115	3416.679250	22.776986
96.379077	3426.511347	22.782003
96.382688	3435.502283	22.787021
96.571529	3454.494714	22.792039
97.105433	3459.389450	22.797056
96.570812	3452.600332	22.802074
97.285419	3453.619608	22.807091
97.128582	3471.849511	22.812109
97.368177	3475.041338	22.817127
97.334479	3469.414301	22.822144
97.408867	3472.465713	22.827162
97.743159	3471.283699	22.832179
97.605644	3482.411331	22.837197
98.083618	3485.431096	22.842215
98.517496	3490.817166	22.847232
98.541134	3496.265120	22.852250
98.621972	3488.906578	22.857267
98.357385	3491.085675	22.862285
99.009833	3486.590509	22.867303
98.907466	3485.940482	22.872320
98.862840	3473.578746	22.877338
98.911855	3462.590891	22.882355
98.572706	3477.717911	22.887373
98.926264	3483.244019	22.892391
98.974593	3482.866331	22.897408
99.140433	3492.206471	22.902426
99.296076	3478.390007	22.907443
99.134858	3492.886863	22.912461
99.214755	3484.562352	22.917479
99.053785	3496.768263	22.922496
99.327990	3513.728976	22.927514
99.144426	3514.384079	22.932531
99.476039	3523.967314	22.937549
99.690694	3539.588309	22.942567
99.806411	3547.979690	22.947584
99.718751	3551.048446	22.952602
100.057199	3536.398977	22.957619
99.816070	3558.386956	22.962637
100.093592	3564.900451	22.967655
100.264130	3572.069414	22.972672
100.422983	3575.245864	22.977690
100.721650	3571.578811	22.982707
100.427665	3591.494490	22.987725
100.990448	3595.245926	22.992743
101.188464	3592.050219	22.997760
101.309305	3593.477853	23.002778
101.472685	3594.583893	23.007795
101.487843	3598.363221	23.012813
101.613977	3596.558119	23.017831
101.518375	3589.005065	23.022848
101.570357	3585.806325	23.027866
101.589261	3586.302386	23.032883
101.407038	3599.121725	23.037901
101.853522	3589.407462	23.042919
101.852055	3601.467021	23.047936
101.620350	3619.542540	23.052954
102.219514	3614.760870	23.057971
101.900167	3626.517465	23.062989
102.019863	3623.300048	23.068007
102.457591	3637.543346	23.073024
102.049638	3645.557141	23.078042
102.531475	3652.953047	23.083059
102.736340	3655.336483	23.088077
102.729848	3652.993843	23.093095
102.692509	3660.218457	23.098112
102.626266	3670.238389	23.103130
103.172434	3677.160294	23.108147
103.121720	3688.697745	23.113165
103.253459	3676.167728	23.118183
103.491091	3683.465027	23.123200
103.519344	3697.394939	23.128218
104.144301	3700.924317	23.133235
104.104246	3701.415163	23.138253
104.381482	3696.407531	23.143271
104.318324	3693.616376	23.148288
104.067107	3704.878310	23.153306
104.248753	3696.499078	23.158323
104.061405	3696.179225	23.163341
104.397546	3689.983124	23.168359
104.684819	3689.550200	23.173376
104.622850	3724.201690	23.178394
104.917514	3721.345498	23.183411
105.095072	3727.776761	23.188429
105.097526	3715.549178	23.193447
105.199940	3720.811753	23.198464
104.920828	3733.016504	23.203482
105.248505	3720.504470	23.208499
105.132003	3719.248501	23.213517
105.225805	3743.621160	23.218535
105.824273	3751.559260	23.223552
105.454583	3758.540017	23.228570
105.568964	3749.339981	23.233587
105.523326	3765.468781	23.238605
105.763195	3766.670463	23.243623
106.187177	3767.457076	23.248640
106.054153	3776.077084	23.253658
106.291718	3771.677166	23.258675
106.256230	3791.570466	23.263693
106.392144	3791.862946	23.268711
106.594896	3803.835767	23.273728
106.540632	3812.295537	23.278746
106.858640	3806.939004	23.283763
107.091428	3812.170225	23.288781
106.759461	3818.464851	23.293799
107.372208	3832.056570	23.298816
107.392324	3840.132015	23.303834
107.502622	3827.547152	23.308851
107.179756	3829.944587	23.313869
107.538287	3824.771905	23.318887
107.595907	3843.184917	23.323904
107.658601	3853.752563	23.328922
108.419383	3856.193778	23.333939
108.053497	3849.106522	23.338957
108.122794	3868.493233	23.343975
108.248771	3858.797117	23.348992
108.326664	3869.946520	23.354010
108.161408	3861.194990	23.359027
108.746321	3868.786963	23.364045
108.745955	3875.987457	23.369063
108.653227	3877.633085	23.374080
108.711328	3873.463975	23.379098
108.759606	3869.977991	23.384115
108.630495	3870.911908	23.389133
108.787483	3901.814590	23.394151
109.006912	3899.691672	23.399168
109.160304	3915.304664	23.404186
109.150491	3914.163729	23.409203
109.358964	3913.007198	23.414221
109.778041	3932.088944	23.419239
109.979900	3930.105148	23.424256
109.854423	3941.326002	23.429274
110.274665	3938.862413	23.434291
110.157012	3941.099182	23.439309
110.075430	3953.296663	23.444327
110.566965	3964.381721	23.449344
110.426970	3970.797051	23.454362
110.779161	3961.042626	23.459379
110.806954	3962.271099	23.464397
110.657455	3965.218262	23.469415
110.864400	3960.634765	23.474432
110.763341	3978.731239	23.479450
111.188965	3982.952293	23.484467
111.360273	3984.983838	23.489485
111.163426	3989.313261	23.494503
111.520331	3984.063629	23.499520
111.842467	3997.833044	23.504538
111.767384	4008.957823	23.509555
112.011510	4008.508398	23.514573
111.979896	4018.702363	23.519591
112.277205	4009.306196	23.524608
112.063547	4019.321183	23.529626
112.317528	4013.512159	23.534643
112.386778	4020.051599	23.539661
112.392504	4038.123410	23.544679
112.426523	4031.835362	23.549696
112.526986	4026.340682	23.554714
112.740521	4046.556553	23.559731
112.844925	4055.192209	23.564749
113.006760	4076.046989	23.569767
113.411242	4073.700947	23.574784
112.873289	4092.939847	23.579802
113.261159	4084.016084	23.584819
113.664816	4088.825062	23.589837
113.344197	4111.729339	23.594855
113.795138	4098.500948	23.599872
113.652251	4102.594315	23.604890
113.994982	4094.578419	23.609907
114.170791	4122.500408	23.614925
113.978139	4132.114349	23.619943
114.352938	4124.331728	23.624960
114.503950	4135.900746	23.629978
114.530748	4143.264202	23.634995
114.740677	4140.868799	23.640013
114.699737	4158.332303	23.645031
114.981807	4154.482813	23.650048
115.010906	4155.968179	23.655066
115.327851	4155.277578	23.660083
115.570441	4149.665274	23.665101
115.548496	4151.430734	23.670119
115.810868	4146.318325	23.675136
115.510585	4148.615617	23.680154
115.770468	4158.442208	23.685171
115.854307	4169.522337	23.690189
116.130478	4178.602133	23.695207
116.411788	4178.460743	23.700224
116.427536	4182.624772	23.705242
116.113027	4167.067222	23.710259
116.221329	4171.237215	23.715277
116.232512	4172.426715	23.720295
116.582774	4184.278997	23.725312
116.583354	4192.280291	23.730330
116.263295	4200.448354	23.735347
116.782893	4196.802526	23.740365
116.703705	4204.251242	23.745383
116.989755	4216.074393	23.750400
117.311422	4228.018050	23.755418
117.344409	4231.111493	23.760435
117.666229	4220.011489	23.765453
117.153159	4239.819310	23.770471
117.657406	4249.542980	23.775488
117.697984	4253.740328	23.780506
117.908240	4244.791489	23.785523
118.104966	4249.005556	23.790541
118.440051	4275.563662	23.795559
118.529033	4279.652228	23.800576
118.695579	4283.485450	23.805594
118.726691	4278.730514	23.810611
118.943165	4279.189226	23.815629
118.774478	4271.790441	23.820647
118.864256	4274.992229	23.825664
119.365021	4286.809090	23.830682
119.083635	4290.779324	23.835699
119.431707	4296.226708	23.840717
119.278064	4305.599655	23.845735
119.197169	4299.678531	23.850752
119.521941	4303.255684	23.855770
119.434493	4318.591542	23.860787
119.718368	4322.707760	23.865805
119.781470	4328.038064	23.870823
120.283391	4337.790127	23.875840
120.453180	4342.455144	23.880858
120.308303	4360.562846	23.885875
120.887929	4359.318969	23.890893
120.482665	4345.801121	23.895911
120.449620	4352.737539	23.900928
120.810860	4362.968001	23.905946
121.025870	4380.646559	23.910963
121.179631	4381.038862	23.915981
120.969205	4380.557446	23.920999
121.289330	4391.179775	23.926016
121.761918	4401.985589	23.931034
121.785368	4412.350248	23.936051
122.349479	4406.222501	23.941069
122.137865	4403.229361	23.946087
122.519463	4402.405227	23.951104
122.409388	4401.922977	23.956122
122.346800	4402.884518	23.961139
122.300888	4401.075074	23.966157
122.191838	4408.932383	23.971175
122.389530	4422.699115	23.976192
122.774183	4430.487850	23.981210
122.644627	4436.866999	23.986227
123.094157	4427.410781	23.991245
123.074721	4441.327980	23.996263
123.062495	4450.863088	24.001280
123.603872	4458.923593	24.006298
123.479564	4457.350728	24.011315
123.576718	4462.463630	24.016333
123.335046	4464.166216	24.021351
123.625766	4484.726613	24.026368
123.842977	4491.737496	24.031386
123.956368	4500.808156	24.036403
123.886525	4493.614990	24.041421
123.951567	4498.081604	24.046439
124.224635	4511.245379	24.051456
124.529880	4515.865230	24.056474
124.647420	4520.085762	24.061491
125.009764	4508.874128	24.066509
124.606763	4519.673515	24.071527
125.056737	4534.920390	24.076544
125.174775	4535.036697	24.081562
125.226129	4554.978830	24.086579
125.395978	4537.224623	24.091597
125.501972	4553.994572	24.096615
125.568542	4547.213117	24.101632
125.846155	4568.173054	24.106650
125.534523	4573.757104	24.111667
126.237322	4574.347290	24.116685
125.798004	4570.603905	24.121703
125.917343	4594.597672	24.126720
126.203558	4597.261136	24.131738
126.321728	4601.167788	24.136755
126.570203	4598.787602	24.141773
126.694407	4617.646459	24.146791
127.046632	4627.356508	24.151808
126.963591	4623.723541	24.156826
126.900897	4631.703231	24.161843
127.386937	4636.671219	24.166861
127.284398	4656.357793	24.171879
127.538130	4657.981690	24.176896
128.027616	4645.923311	24.181914
127.998171	4650.434322	24.186931
128.185832	4649.094159	24.191949
128.158522	4659.465007	24.196967
128.399273	4663.847119	24.201984
128.993648	4669.338195	24.207002
128.686232	4680.970374	24.212019
129.107433	4666.434135	24.217037
129.183080	4663.132833	24.222055
128.874465	4666.849377	24.227072
129.140856	4667.486086	24.232090
129.177762	4657.625835	24.237107
129.637424	4665.711761	24.242125
129.106580	4668.835854	24.247143
129.786232	4679.150534	24.252160
129.668444	4693.539748	24.257178
129.605683	4693.961144	24.262195
129.614267	4687.602226	24.267213
129.831195	4710.051607	24.272231
129.729913	4728.948250	24.277248
130.231056	4716.948918	24.282266
130.615659	4731.383508	24.287283
130.387637	4725.792457	24.292301
130.570829	4747.503324	24.297319
130.685366	4751.654332	24.302336
130.884554	4742.905869	24.307354
130.579316	4761.444889	24.312371
130.824907	4769.189052	24.317389
131.342217	4778.332512	24.322407
131.106701	4785.369512	24.327424
131.416649	4795.008300	24.332442
131.391174	4807.066460	24.337459
131.310190	4814.992962	24.342477
131.631743	4823.801840	24.347495
131.848794	4835.698286	24.352512
132.081557	4838.627728	24.357530
132.031961	4856.757271	24.362547
132.498788	4865.008666	24.367565
132.999899	4873.813496	24.372583
132.878195	4868.762741	24.377600
133.253207	4860.400939	24.382618
132.900310	4869.450035	24.387635
133.676752	4857.753557	24.392653
133.761187	4864.436522	24.397671
133.523883	4859.498972	24.402688
133.935779	4855.090026	24.407706
133.656392	4863.653710	24.412723
133.701281	4882.066511	24.417741
133.855983	4883.444572	24.422759
133.947528	4888.768399	24.427776
134.254723	4890.140556	24.432794
134.238166	4896.025595	24.437811
134.446015	4906.392006	24.442829
134.385919	4922.238936	24.447847
134.204905	4932.535355	24.452864
134.366627	4918.650860	24.457882
134.517158	4949.486209	24.462899
134.672142	4955.703978	24.467917
135.275946	4954.442677	24.472935
135.191802	4986.460667	24.477952
135.493358	4986.328526	24.482970
135.754543	4975.721904	24.487987
135.758652	5001.194508	24.493005
135.835584	5009.033987	24.498023
135.945196	5000.867945	24.503040
136.356968	5004.315916	24.508058
136.133878	5021.396671	24.513075
136.417459	5034.300469	24.518093
136.936460	5032.610225	24.523111
136.736293	5040.647487	24.528128
137.069740	5026.187231	24.533146
137.197335	5040.717336	24.538163
137.323081	5046.880125	24.543181
137.584009	5051.984665	24.548199
137.718942	5054.441690	24.553216
138.093821	5054.276959	24.558234
137.888570	5053.101693	24.563251
137.985618	5058.546726	24.568269
138.040290	5064.214136	24.573287
138.298174	5082.231318	24.578304
138.522481	5084.263308	24.583322
138.364272	5086.488042	24.588339
138.571246	5082.231801	24.593357
138.789837	5096.437052	24.598375
138.711009	5121.994823	24.603392
138.752783	5116.728376	24.608410
138.762366	5127.365116	24.613427
139.281978	5135.612265	24.618445
139.651514	5144.185424	24.623463
139.548402	5157.391036	24.628480
139.629264	5148.270131	24.633498
139.687496	5161.150241	24.638515
139.473322	5166.470342	24.643533
139.923972	5171.500263	24.648551
139.643575	5186.205407	24.653568
140.187037	5192.307501	24.658586
140.136991	5202.977770	24.663603
140.252229	5205.597930	24.668621
140.515626	5224.520750	24.673639
141.066892	5226.941690	24.678656
141.217387	5229.437907	24.683674
141.232385	5245.115261	24.688691
141.250321	5257.937143	24.693709
141.221271	5259.611767	24.698727
141.601423	5271.256771	24.703744
142.003997	5271.588694	24.708762
141.653219	5274.368158	24.713779
142.041041	5278.382409	24.718797
142.113341	5275.852081	24.723815
142.469168	5283.666483	24.728832
142.783494	5286.225412	24.733850
143.119231	5298.151818	24.738867
142.906483	5312.793141	24.743885
142.954394	5296.953688	24.748903
143.079938	5309.493238	24.753920
143.385168	5301.262430	24.758938
143.185894	5305.062641	24.763955
143.070186	5323.626132	24.768973
143.358733	5328.386402	24.773991
143.452601	5333.389885	24.779008
143.660848	5339.821077	24.784026
143.901362	5361.830051	24.789043
143.965686	5372.183869	24.794061
144.451605	5368.633901	24.799079
144.448043	5382.594201	24.804096
144.995841	5376.405383	24.809114
145.155022	5386.012357	24.814131
145.205682	5383.880511	24.819149
145.585838	5379.894031	24.824167
145.652580	5387.703491	24.829184
145.685812	5377.827643	24.834202
145.864285	5379.269545	24.839219
145.762940	5386.602000	24.844237
146.103648	5389.729089	24.849255
146.043811	5409.645799	24.854272
146.361174	5408.571181	24.859290
146.100073	5411.577610	24.864307
146.082332	5421.169739	24.869325
146.558674	5418.735243	24.874343
146.591343	5440.352247	24.879360
146.576013	5441.823421	24.884378
146.828481	5445.567136	24.889395
146.844705	5475.344888	24.894413
147.142420	5466.702591	24.899431
146.963811	5487.056394	24.904448
147.410546	5488.317352	24.909466
147.765221	5497.733807	24.914483
147.448792	5502.545661	24.919501
148.022522	5518.038438	24.924519
148.189285	5530.525286	24.929536
148.147593	5525.183506	24.934554
148.468362	5526.772796	24.939571
148.492266	5547.786996	24.944589
149.204155	5546.720811	24.949607
148.927740	5553.134917	24.954624
149.410070	5547.385641	24.959642
149.559385	5544.820494	24.964659
149.635604	5553.113566	24.969677
150.073099	5558.171774	24.974695
149.990479	5567.287255	24.979712
150.041421	5571.430876	24.984730
150.311387	5575.159525	24.989747
149.929092	5567.899761	24.994765
150.360702	5564.320924	24.999783
150.369147	5579.716986	25.004800
150.600559	5586.169651	25.009818
150.689274	5600.104661	25.014835
150.978971	5592.610213	25.019853
151.033122	5599.073274	25.024871
151.026302	5615.575174	25.029888
151.274411	5625.614113	25.034906
151.171480	5626.886761	25.039923
151.113005	5640.589009	25.044941
151.439361	5652.712930	25.049959
151.565605	5666.276398	25.054976
151.638466	5684.763878	25.059994
151.805609	5695.723833	25.065011
151.805064	5701.122610	25.070029
152.353147	5700.602838	25.075047
152.515594	5715.166399	25.080064
152.548369	5729.923468	25.085082
153.050090	5725.128920	25.090099
152.735750	5749.102405	25.095117
153.351133	5749.385397	25.100135
153.361956	5740.273358	25.105152
153.267515	5749.265291	25.110170
153.849411	5767.097820	25.115187
153.870098	5770.168007	25.120205
154.154820	5779.476491	25.125223
154.471419	5768.571952	25.130240
154.463237	5766.072561	25.135258
154.785545	5782.425361	25.140275
154.514370	5795.567535	25.145293
155.039183	5803.989008	25.150311
154.997202	5807.858638	25.155328
154.955324	5808.061623	25.160346
155.160104	5814.342382	25.165363
155.058966	5840.820488	25.170381
155.640716	5830.956887	25.175399
155.505166	5840.953830	25.180416
155.623358	5856.828554	25.185434
155.985880	5857.735298	25.190451
155.977106	5868.899268	25.195469
156.424225	5876.476020	25.200487
156.420935	5888.427789	25.205504
156.088083	5897.193808	25.210522
156.894763	5901.283522	25.215539
156.536005	5929.671926	25.220557
156.937304	5919.542769	25.225575
157.206943	5937.189652	25.230592
157.258599	5950.468011	25.235610
157.546723	5954.470168	25.240627
157.493465	5965.212362	25.245645
157.848304	5972.978449	25.250663
157.870089	5987.311925	25.255680
157.765745	5997.420757	25.260698
158.529867	6004.884948	25.265715
158.499476	6009.386663	25.270733
158.595875	6020.143149	25.275751
159.204327	6031.440324	25.280768
159.353319	6039.432611	25.285786
159.702181	6028.811186	25.290803
159.575117	6033.606875	25.295821
159.970736	6039.914075	25.300839
160.212500	6029.745844	25.305856
159.673031	6042.918773	25.310874
160.267256	6042.264578	25.315891
160.037598	6041.641774	25.320909
160.501743	6042.429754	25.325927
160.667715	6065.708915	25.330944
160.547106	6077.478607	25.335962
160.563949	6084.460314	25.340979
160.661198	6092.655695	25.345997
161.012060	6103.424532	25.351015
161.394751	6112.409894	25.356032
161.227129	6116.095604	25.361050
161.664702	6126.188611	25.366067
161.593735	6144.451147	25.371085
161.893931	6142.142119	25.376103
162.304710	6145.278654	25.381120
162.061900	6166.653549	25.386138
162.724602	6166.790523	25.391155
162.671057	6177.166317	25.396173
162.735264	6168.718936	25.401191
163.013816	6172.556958	25.406208
162.685424	6171.832333	25.411226
163.000121	6188.251392	25.416243
163.463108	6199.742043	25.421261
163.684633	6199.818033	25.426279
163.771699	6198.389228	25.431296
163.950976	6218.432049	25.436314
164.289952	6229.347054	25.441331
164.021970	6230.129223	25.446349
164.279937	6221.591522	25.451367
164.259671	6244.423691	25.456384
164.088649	6256.608999	25.461402
164.983081	6257.707059	25.466419
165.024834	6279.610774	25.471437
165.041920	6279.681167	25.476455
165.007670	6290.187728	25.481472
164.897597	6293.330812	25.486490
165.778573	6311.790642	25.491507
165.912152	6306.439324	25.496525
165.808437	6320.056318	25.501543
166.114403	6337.584246	25.506560
165.934012	6348.640276	25.511578
166.376069	6340.468223	25.516595
166.685691	6363.789456	25.521613
166.926422	6362.860531	25.526631
167.180560	6368.110745	25.531648
167.184575	6386.549394	25.536666
167.445214	6388.653914	25.541683
167.834331	6398.776368	25.546701
167.805810	6398.527471	25.551719
167.934426	6408.197613	25.556736
167.530609	6414.013327	25.561754
168.146757	6430.937258	25.566771
167.931855	6428.209274	25.571789
168.423534	6440.456123	25.576807
168.813907	6456.977940	25.581824
168.585178	6458.919978	25.586842
169.038568	6473.485393	25.591859
169.367074	6486.077404	25.596877
169.433197	6479.517274	25.601895
169.728046	6487.247852	25.606912
169.741682	6508.187069	25.611930
169.874824	6514.354334	25.616947
169.549782	6520.183059	25.621965
169.905381	6538.169236	25.626983
170.188804	6540.708673	25.632000
170.274768	6561.862035	25.637018
170.677114	6563.443075	25.642035
170.750871	6584.737880	25.647053
170.965791	6588.132892	25.652071
171.480564	6589.821365	25.657088
171.339380	6616.156578	25.662106
171.234685	6609.708097	25.667123
171.304321	6627.193493	25.672141
171.712786	6633.073536	25.677159
171.796724	6648.519995	25.682176
172.007514	6671.101968	25.687194
172.353771	6666.862059	25.692212
172.476931	6683.688158	25.697229
172.443542	6703.899045	25.702247
172.762584	6696.686683	25.707264
172.798352	6721.918617	25.712282
173.201598	6736.189353	25.717300
173.682891	6726.371723	25.722317
173.608681	6764.383394	25.727335
174.232544	6754.171252	25.732352
173.964506	6757.088511	25.737370
174.546411	6755.069135	25.742388
174.435113	6755.271001	25.747405
174.423240	6759.480051	25.752423
174.833909	6783.418405	25.757440
175.082003	6783.799519	25.762458
175.059564	6783.589776	25.767476
175.244442	6780.003395	25.772493
175.556124	6794.164880	25.777511
175.821097	6803.926932	25.782528
175.704734	6820.260365	25.787546
175.799503	6814.670358	25.792564
175.992516	6820.944409	25.797581
176.059942	6849.762576	25.802599
176.391956	6835.993162	25.807616
176.495466	6846.685247	25.812634
176.670291	6862.962736	25.817652
176.994797	6883.393516	25.822669
176.388742	6886.928967	25.827687
176.734044	6903.141315	25.832704
176.735198	6920.969914	25.837722
176.812576	6932.794164	25.842740
177.337768	6952.079836	25.847757
177.440175	6967.637753	25.852775
177.978851	6975.914234	25.857792
177.676529	6993.260664	25.862810
178.161791	7002.506027	25.867828
178.676551	7004.727732	25.872845
178.882159	7021.131035	25.877863
179.476288	7021.206110	25.882880
179.325979	7030.714016	25.887898
179.738246	7041.237084	25.892916
180.001434	7044.934522	25.897933
179.683600	7053.699093	25.902951
180.363698	7050.567950	25.907968
180.058362	7073.910725	25.912986
180.371319	7077.058100	25.918004
180.633686	7080.565091	25.923021
180.526073	7095.765625	25.928039
180.798374	7094.117905	25.933056
180.937518	7119.615344	25.938074
181.240630	7131.615090	25.943092
181.552487	7140.263066	25.948109
181.223402	7143.564579	25.953127
181.848543	7169.125925	25.958144
181.725100	7172.080012	25.963162
181.879148	7183.135710	25.968180
182.354685	7201.071326	25.973197
182.303106	7207.662385	25.978215
182.547109	7220.804500	25.983232
182.709641	7228.903054	25.988250
182.757118	7241.027029	25.993268
183.496990	7250.295840	25.998285
183.516962	7259.562315	26.003303
184.003896	7267.100876	26.008320
183.958482	7271.532188	26.013338
184.319819	7284.702225	26.018356
184.847031	7287.558279	26.023373
184.550017	7293.811887	26.028391
184.968427	7290.737325	26.033408
184.942100	7302.641207	26.038426
185.200139	7310.961084	26.043444
185.531567	7326.996594	26.048461
185.281777	7328.413748	26.053479
185.541450	7323.724874	26.058496
185.761803	7339.188849	26.063514
185.817021	7354.907736	26.068532
186.055760	7351.771489	26.073549
185.869109	7361.747123	26.078567
185.970704	7378.704329	26.083584
186.100926	7387.559658	26.088602
186.388293	7412.099005	26.093620
186.650254	7415.756567	26.098637
186.439900	7428.766793	26.103655
186.590819	7437.068207	26.108672
187.200974	7454.083232	26.113690
187.274782	7472.602192	26.118708
187.873551	7472.874979	26.123725
187.576601	7495.143505	26.128743
188.120414	7507.498351	26.133760
188.216159	7511.453543	26.138778
188.901178	7527.415870	26.143796
189.080220	7526.151321	26.148813
189.261167	7533.493263	26.153831
189.430197	7529.362744	26.158848
189.587853	7534.483587	26.163866
189.661424	7557.354134	26.168884
190.319090	7560.658879	26.173901
190.047582	7556.983123	26.178919
190.470094	7551.864816	26.183936
190.534773	7568.415627	26.188954
190.869750	7581.802131	26.193972
190.925202	7576.420762	26.198989
190.887734	7592.912867	26.204007
191.089951	7576.969227	26.209024
191.159821	7589.326049	26.214042
191.457440	7613.029163	26.219060
191.515634	7613.069931	26.224077
191.663038	7643.624798	26.229095
191.991932	7639.098453	26.234112
192.086205	7654.704072	26.239130
192.409559	7682.515091	26.244148
192.727375	7682.803587	26.249165
192.516509	7703.600336	26.254183
192.908613	7706.415784	26.259200
192.929753	7721.737415	26.264218
193.336468	7733.702389	26.269236
193.803677	7743.077189	26.274253
193.635984	7765.657108	26.279271
193.706048	7770.220700	26.284288
193.888744	7778.112215	26.289306
193.918054	7796.697190	26.294324
194.292990	7803.982004	26.299341
194.532485	7834.515723	26.304359
194.840133	7833.775712	26.309376
195.250683	7851.749587	26.314394
194.982052	7871.953580	26.319412
195.466041	7872.672226	26.324429
195.667644	7898.050338	26.329447
195.939677	7900.836040	26.334464
196.311918	7908.538781	26.339482
196.543152	7915.999399	26.344500
196.837466	7925.413114	26.349517
196.604105	7924.897169	26.354535
197.019864	7937.857133	26.359552
197.357878	7947.622005	26.364570
197.424865	7950.464436	26.369588
197.669541	7953.840652	26.374605
197.894337	7967.865541	26.379623
197.909214	7966.819471	26.384640
198.319204	7985.174008	26.389658
198.477148	7999.450193	26.394676
198.798852	8011.584585	26.399693
198.463085	8007.879959	26.404711
198.790928	8025.876361	26.409728
198.738254	8035.716078	26.414746
198.612758	8050.859838	26.419764
199.112738	8077.647608	26.424781
199.278754	8080.812377	26.429799
199.622030	8090.910419	26.434816
199.785703	8109.598793	26.439834
199.904102	8117.390047	26.444852
200.324050	8133.912679	26.449869
200.258265	8148.931674	26.454887
200.400853	8167.961491	26.459904
200.999838	8173.087599	26.464922
201.060761	8194.378033	26.469940
200.942477	8207.213008	26.474957
201.390844	8214.681211	26.479975
201.565767	8224.466113	26.484992
201.974096	8237.370054	26.490010
201.885837	8259.622500	26.495028
202.443186	8269.099291	26.500045
202.521774	8287.091491	26.505063
202.896179	8292.017668	26.510080
203.498195	8280.911839	26.515098
203.390950	8300.803016	26.520116
203.513627	8309.938931	26.525133
203.474979	8312.253840	26.530151
203.653282	8325.701518	26.535168
204.136073	8334.178561	26.540186
204.189438	8349.682931	26.545204
204.462559	8366.007167	26.550221
204.933985	8368.243321	26.555239
205.086734	8375.394982	26.560256
205.447384	8383.771723	26.565274
205.507810	8401.667812	26.570292
206.074920	8411.060375	26.575309
205.986763	8409.849356	26.580327
206.175385	8423.789260	26.585344
206.314019	8424.553968	26.590362
205.859665	8444.385318	26.595380
206.208307	8443.501459	26.600397
206.420677	8457.536712	26.605415
206.756974	8487.172754	26.610432
207.072173	8493.224075	26.615450
207.295486	8518.774452	26.620468
207.509378	8527.153463	26.625485
207.639132	8536.106395	26.630503
207.636122	8551.947149	26.635520
208.316997	8570.798722	26.640538
208.378751	8587.963081	26.645556
208.637743	8585.476992	26.650573
208.920807	8610.852240	26.655591
208.481956	8634.001191	26.660608
209.185330	8640.320033	26.665626
209.148856	8652.907920	26.670644
209.363362	8674.406767	26.675661
209.763962	8684.045970	26.680679
210.105205	8697.258316	26.685696
210.776225	8705.517786	26.690714
210.605289	8715.108874	26.695732
210.566900	8721.816530	26.700749
211.181041	8735.642296	26.705767
211.311542	8743.468879	26.710784
211.304319	8758.668599	26.715802
211.449343	8779.291382	26.720820
211.862123	8782.455692	26.725837
211.829225	8804.150759	26.730855
211.916398	8810.580932	26.735872
212.661090	8829.187548	26.740890
212.525367	8844.009238	26.745908
212.740989	8851.213739	26.750925
213.220367	8862.190081	26.755943
213.027396	8879.620536	26.760960
213.491693	8890.939659	26.765978
213.567787	8907.930285	26.770996
213.978547	8905.703417	26.776013
214.071315	8909.562569	26.781031
214.368474	8926.047244	26.786048
214.759751	8929.556982	26.791066
214.658548	8935.814325	26.796084
214.823833	8958.628420	26.801101
215.052253	8958.419734	26.806119
215.116138	8981.616880	26.811136
215.476595	8992.235670	26.816154
215.321142	9004.062129	26.821172
215.753985	9024.095763	26.826189
216.165593	9033.682951	26.831207
216.279269	9054.076547	26.836224
216.759055	9051.519249	26.841242
216.476752	9074.190854	26.846260
216.620107	9090.324605	26.851277
217.119344	9105.711937	26.856295
217.034947	9117.153385	26.861312
217.650386	9138.787474	26.866330
217.805625	9161.503487	26.871348
217.760276	9174.444555	26.876365
218.324461	9186.257011	26.881383
217.924694	9210.655895	26.886400
218.761821	9215.689440	26.891418
219.103725	9233.038210	26.896436
219.051391	9253.209795	26.901453
219.534814	9258.404979	26.906471
220.104427	9278.126472	26.911488
220.271573	9272.587444	26.916506
220.455555	9280.811110	26.921524
220.505799	9300.256108	26.926541
220.710050	9306.824674	26.931559
220.618874	9320.235013	26.936576
221.300078	9331.327208	26.941594
221.303860	9343.582891	26.946612
221.690517	9357.469629	26.951629
222.058354	9365.708649	26.956647
221.817255	9375.905640	26.961664
222.360228	9387.790280	26.966682
222.524362	9402.622024	26.971700
222.748139	9414.892613	26.976717
222.988925	9425.817396	26.981735
222.983397	9432.860991	26.986752
223.209535	9449.857337	26.991770
223.734807	9455.520648	26.996788
223.768199	9478.310808	27.001805
223.946786	9480.666400	27.006823
224.408753	9502.267266	27.011840
224.891967	9517.860083	27.016858
224.997086	9534.785931	27.021876
224.979018	9534.966911	27.026893
225.363096	9542.237630	27.031911
225.178591	9563.426300	27.036928
225.697843	9571.355265	27.041946
225.795477	9592.279955	27.046964
225.901062	9591.577193	27.051981
226.015771	9598.445032	27.056999
226.132288	9619.016113	27.062016
226.489792	9634.304496	27.067034
226.936573	9653.702527	27.072052
227.166457	9664.071586	27.077069
227.571878	9678.606145	27.082087
227.316130	9696.139237	27.087104
227.609842	9719.479869	27.092122
227.838509	9724.830727	27.097140
227.854199	9749.538313	27.102157
228.211324	9752.315802	27.107175
228.423048	9789.246927	27.112192
228.545301	9789.475619	27.117210
228.979293	9816.124418	27.122228
229.007542	9816.534848	27.127245
229.178200	9833.466726	27.132263
229.542704	9856.999880	27.137280
230.274594	9865.270385	27.142298
230.367733	9867.784304	27.147316
230.389442	9882.094932	27.152333
230.859308	9883.613964	27.157351
231.022502	9897.010331	27.162368
231.882135	9890.874599	27.167386
231.379256	9918.666933	27.172404
231.607145	9924.247212	27.177421
231.862222	9926.151479	27.182439
232.256176	9952.010744	27.187456
232.587110	9950.261675	27.192474
232.704986	9964.631322	27.197492
233.104037	9975.746169	27.202509
233.189601	9976.647331	27.207527
233.338218	10006.387323	27.212544
233.261219	10010.600118	27.217562
233.575719	10032.956283	27.222580
233.508640	10053.590555	27.227597
234.212113	10071.257032	27.232615
234.350523	10093.792041	27.237632
234.455421	10105.793712	27.242650
234.716432	10127.293929	27.247668
234.804390	10143.568663	27.252685
235.052500	10161.305748	27.257703
235.173989	10186.169828	27.262720
235.359075	10205.679514	27.267738
235.625139	10218.726735	27.272756
235.618464	10255.449252	27.277773
235.944309	10274.034606	27.282791
236.443745	10296.074638	27.287808
236.799096	10305.879853	27.292826
237.073654	10334.960012	27.297844
237.401861	10349.492187	27.302861
237.999618	10355.565284	27.307879
238.446399	10371.339048	27.312896
238.992783	10372.231055	27.317914
239.300835	10379.307546	27.322932
239.140330	10391.892091	27.327949
239.558046	10411.472301	27.332967
239.624422	10401.535854	27.337984
239.562706	10417.235341	27.343002
239.812093	10426.663483	27.348020
240.097625	10436.408629	27.353037
240.499599	10448.870353	27.358055
240.226020	10467.844855	27.363072
240.289092	10488.781158	27.368090
240.804522	10502.256116	27.373108
240.721397	10516.862705	27.378125
241.366144	10517.539960	27.383143
241.983379	10553.837108	27.388160
242.013677	10558.330086	27.393178
242.368882	10566.938906	27.398196
242.351280	10583.974370	27.403213
242.994343	10595.673228	27.408231
242.631382	10613.874138	27.413248
243.164829	10625.129511	27.418266
243.398880	10639.918557	27.423284
243.445389	10665.036821	27.428301
243.871579	10667.004286	27.433319
244.205710	10685.036539	27.438336
244.274573	10685.066101	27.443354
244.731759	10708.092068	27.448372
245.145076	10720.469418	27.453389
245.114544	10722.128714	27.458407
245.300837	10746.533942	27.463424
245.799308	10745.491294	27.468442
245.831292	10743.918361	27.473460
246.021177	10777.572821	27.478477
246.421854	10772.382267	27.483495
246.521419	10789.603407	27.488512
246.546982	10808.777031	27.493530
246.978418	10811.590485	27.498548
246.802064	10837.798280	27.503565
247.128754	10856.255768	27.508583
247.308769	10880.276236	27.513600
247.551994	10894.108452	27.518618
247.914906	10912.773504	27.523636
247.973208	10928.805791	27.528653
248.183776	10948.051425	27.533671
248.098802	10969.446872	27.538688
248.546727	10995.663646	27.543706
248.886987	11018.314709	27.548724
249.170699	11048.407719	27.553741
249.840281	11061.162873	27.558759
249.861290	11078.935348	27.563776
249.933791	11105.390788	27.568794
250.799416	11125.453250	27.573812
250.973887	11141.754094	27.578829
251.330841	11165.305392	27.583847
251.345383	11182.816722	27.588864
251.598332	11196.616082	27.593882
251.985551	11202.734531	27.598900
251.975972	11226.934944	27.603917
252.305646	11235.777587	27.608935
252.481635	11263.991836	27.613952
252.908282	11278.557436	27.618970
253.224647	11305.651980	27.623988
253.206722	11321.259249	27.629005
253.759569	11340.058065	27.634023
254.264026	11339.885679	27.639040
254.068279	11370.237334	27.644058
254.621256	11376.708176	27.649076
254.866327	11393.668015	27.654093
255.137734	11401.383604	27.659111
255.252443	11430.956170	27.664128
255.289975	11445.730374	27.669146
255.602853	11454.005556	27.674164
255.681412	11481.825061	27.679181
256.128153	11504.919288	27.684199
256.713587	11527.052376	27.689216
256.702377	11539.512316	27.694234
257.248899	11552.583618	27.699252
257.527838	11574.282130	27.704269
257.723037	11593.360127	27.709287
257.612460	11597.335457	27.714304
257.939319	11615.250215	27.719322
258.643842	11635.958355	27.724340
258.586609	11661.942198	27.729357
258.559732	11665.883234	27.734375
259.188718	11689.588884	27.739392
259.458400	11703.600985	27.744410
259.829133	11714.448359	27.749428
260.003522	11733.763149	27.754445
260.283659	11758.125263	27.759463
260.446073	11768.758934	27.764480
260.381198	11786.040611	27.769498
260.799808	11808.983151	27.774516
260.943728	11826.559678	27.779533
261.126041	11841.375714	27.784551
261.554487	11863.788878	27.789568
261.528669	11881.773231	27.794586
262.140907	11890.311939	27.799604
262.407525	11911.370092	27.804621
262.540840	11939.429502	27.809639
262.844823	11942.996880	27.814656
262.891649	11960.140542	27.819674
263.606907	11975.634404	27.824692
263.866185	11991.050780	27.829709
264.045354	11995.785058	27.834727
264.439121	12020.612515	27.839744
264.187330	12033.662478	27.844762
264.883387	12047.278281	27.849780
265.159784	12066.302459	27.854797
265.483002	12080.656622	27.859815
265.512386	12100.114770	27.864832
266.031841	12118.951531	27.869850
265.940973	12112.536346	27.874868
266.196539	12152.746153	27.879885
266.788822	12166.154674	27.884903
267.076642	12182.247195	27.889920
267.044577	12206.983001	27.894938
267.456969	12217.815167	27.899956
267.954568	12249.973855	27.904973
267.930744	12256.792456	27.909991
268.240295	12271.262495	27.915008
268.167082	12290.635406	27.920026
268.638778	12315.733273	27.925044
268.767327	12345.113789	27.930061
269.109092	12362.037405	27.935079
269.474820	12388.805762	27.940096
269.671564	12395.504470	27.945114
270.294091	12428.902620	27.950132
270.236179	12447.606683	27.955149
270.572440	12464.890569	27.960167
270.908443	12484.642020	27.965184
270.887277	12517.614909	27.970202
271.649619	12523.943697	27.975220
271.718489	12553.523534	27.980237
271.601438	12561.224290	27.985255
272.400340	12583.708036	27.990272
272.348921	12615.888041	27.995290
272.894381	12628.092983	28.000308
273.270230	12651.997082	28.005325
273.492055	12668.130143	28.010343
274.069224	12692.183822	28.015360
274.002291	12709.702394	28.020378
274.072566	12728.692077	28.025396
274.501348	12747.455530	28.030413
274.737985	12760.472655	28.035431
274.860357	12781.015312	28.040448
275.173542	12822.576313	28.045466
275.312392	12833.323304	28.050484
275.934391	12852.543426	28.055501
276.223984	12877.632862	28.060519
276.551015	12886.881812	28.065536
276.479063	12920.149118	28.070554
276.843074	12934.533546	28.075572
276.955655	12956.658487	28.080589
276.908334	12987.419620	28.085607
277.614247	13009.820055	28.090624
277.760883	13035.283165	28.095642
278.443567	13055.355427	28.100660
278.662835	13076.652982	28.105677
278.802061	13103.444189	28.110695
279.802653	13111.524672	28.115712
279.469716	13133.463464	28.120730
279.746703	13149.397228	28.125748
279.957338	13161.738255	28.130765
280.180638	13185.394169	28.135783
280.820763	13192.829890	28.140800
280.975875	13213.760048	28.145818
281.491864	13235.368061	28.150836
281.435450	13243.971480	28.155853
281.546700	13260.611883	28.160871
282.138321	13278.143603	28.165888
282.657352	13298.662355	28.170906
282.934443	13302.467692	28.175924
283.040507	13316.586230	28.180941
282.723617	13354.767127	28.185959
283.414606	13353.345066	28.190976
283.457484	13384.944537	28.195994
284.053511	13399.005836	28.201012
283.918580	13427.396574	28.206029
284.162983	13444.640747	28.211047
284.524806	13471.469849	28.216064
284.767437	13498.105959	28.221082
284.925745	13518.192944	28.226100
285.048146	13550.680942	28.231117
285.678446	13584.530086	28.236135
286.384295	13590.157169	28.241152
285.996274	13617.759617	28.246170
286.465712	13638.216084	28.251188
286.826063	13658.819813	28.256205
287.242368	13679.130683	28.261223
287.908455	13706.363734	28.266240
287.938958	13732.600356	28.271258
288.246100	13748.063294	28.276276
288.905239	13758.360935	28.281293
288.713182	13809.417029	28.286311
288.994989	13819.030117	28.291328
289.370209	13840.430554	28.296346
289.563639	13863.528256	28.301364
289.881107	13881.397449	28.306381
290.200439	13916.248875	28.311399
290.590394	13939.604167	28.316416
290.942157	13959.179115	28.321434
291.285100	13976.626613	28.326452
291.647708	14004.367292	28.331469
291.631587	14025.225935	28.336487
292.222895	14048.557573	28.341504
292.412019	14068.443172	28.346522
292.642685	14088.312476	28.351540
292.689959	14120.763601	28.356557
292.797794	14142.750697	28.361575
293.674605	14153.239550	28.366592
293.683800	14176.467413	28.371610
294.042968	14202.880568	28.376628
294.084417	14222.278604	28.381645
294.011979	14245.092997	28.386663
294.872715	14275.955537	28.391680
294.917066	14303.413650	28.396698
295.193212	14312.356655	28.401716
295.728375	14354.176446	28.406733
295.765884	14386.412246	28.411751
296.428974	14407.220626	28.416768
296.704310	14434.164890	28.421786
296.859356	14453.782389	28.426804
297.100088	14482.847261	28.431821
297.662630	14512.741506	28.436839
297.876826	14526.431930	28.441856
298.085803	14554.898617	28.446874
298.693136	14586.728652	28.451892
298.787061	14607.119159	28.456909
298.861083	14626.679338	28.461927
299.391254	14644.296761	28.466944
299.712166	14683.492705	28.471962
299.921270	14692.443844	28.476980
300.342895	14705.865344	28.481997
300.276193	14731.965200	28.487015
300.754629	14752.747798	28.492032
301.110788	14764.736643	28.497050
301.147365	14792.638116	28.502068
301.446154	14813.929544	28.507085
301.416021	14846.432725	28.512103
301.760377	14875.191212	28.517120
302.084498	14901.866590	28.522138
302.772242	14933.275859	28.527156
303.651170	14948.305082	28.532173
303.656484	14980.290502	28.537191
303.837408	15004.315378	28.542208
304.319659	15012.944207	28.547226
304.635691	15035.591518	28.552244
304.921008	15061.651081	28.557261
305.109430	15089.330985	28.562279
305.428776	15102.006961	28.567296
305.938486	15126.220392	28.572314
305.903143	15157.834654	28.577332
306.386086	15160.153415	28.582349
306.564936	15199.942983	28.587367
306.906192	15223.511463	28.592384
307.151276	15245.847721	28.597402
307.421970	15267.394958	28.602420
308.025851	15291.892506	28.607437
308.123261	15311.164397	28.612455
308.464452	15327.009322	28.617472
308.698248	15360.062480	28.622490
309.083112	15381.776969	28.627508
309.649580	15407.863131	28.632525
309.731132	15430.877529	28.637543
310.121549	15454.884218	28.642560
310.958902	15472.908821	28.647578
310.980226	15488.783108	28.652596
311.707287	15491.189241	28.657613
311.514301	15521.736531	28.662631
312.241223	15539.212103	28.667648
312.336818	15557.882565	28.672666
312.635316	15573.257264	28.677684
312.850600	15592.358720	28.682701
312.689730	15621.684239	28.687719
313.488818	15632.694364	28.692736
313.461987	15664.667523	28.697754
313.770733	15693.589359	28.702772
313.880223	15712.932224	28.707789
314.149316	15753.537201	28.712807
314.771139	15775.167364	28.717824
315.289061	15801.200712	28.722842
315.200378	15824.817450	28.727860
315.646410	15843.488655	28.732877
316.012671	15879.997634	28.737895
316.298319	15912.137142	28.742912
316.474401	15932.019290	28.747930
316.419212	15961.753479	28.752948
316.803685	15987.123607	28.757965
317.121433	16011.362186	28.762983
317.757062	16049.630003	28.768000
317.979956	16084.368038	28.773018
318.228538	16112.132722	28.778036
318.887557	16144.360725	28.783053
318.843711	16172.243166	28.788071
318.788480	16200.442742	28.793088
319.568599	16219.152171	28.798106
320.318133	16253.059672	28.803124
320.834959	16277.267333	28.808141
321.051507	16294.790209	28.813159
321.391597	16318.095687	28.818176
322.024728	16324.553717	28.823194
321.969023	16338.294980	28.828212
322.608037	16352.933307	28.833229
322.486508	16364.970727	28.838247
322.839430	16376.666575	28.843264
323.478047	16402.296386	28.848282
323.468110	16412.345341	28.853300
324.040316	16439.399902	28.858317
324.230763	16457.819311	28.863335
324.036031	16485.720908	28.868352
324.838177	16502.244180	28.873370
325.019057	16532.923869	28.878388
325.258493	16553.157223	28.883405
325.582122	16584.963955	28.888423
326.060737	16589.296283	28.893440
326.339112	16626.094105	28.898458
326.595906	16653.097105	28.903476
326.904696	16669.851779	28.908493
327.109785	16707.465691	28.913511
327.199140	16731.453068	28.918528
327.779232	16762.554245	28.923546
328.268507	16781.734759	28.928564
328.833124	16801.943070	28.933581
328.993806	16832.560459	28.938599
328.942342	16857.605202	28.943616
329.551585	16883.845842	28.948634
329.712276	16909.498664	28.953652
330.146172	16928.567140	28.958669
330.396272	16961.890351	28.963687
330.451036	16994.998451	28.968704
331.162316	17020.327223	28.973722
331.201695	17059.175040	28.978740
331.738842	17076.768725	28.983757
332.104371	17107.575017	28.988775
332.374544	17146.911338	28.993792
332.616422	17172.568495	28.998810
332.896287	17206.966932	29.003828
333.620095	17224.832556	29.008845
334.189317	17258.540237	29.013863
334.178107	17281.542609	29.018880
334.778944	17306.012160	29.023898
334.942952	17350.771088	29.028916
335.347730	17365.734302	29.033933
335.610647	17394.346753	29.038951
335.855251	17422.111158	29.043968
336.396101	17445.619919	29.048986
336.524570	17470.900663	29.054004
336.971901	17489.291401	29.059021
337.268255	17529.073514	29.064039
337.146743	17552.252102	29.069056
338.067587	17573.231576	29.074074
338.102951	17610.656504	29.079092
338.267579	17635.950442	29.084109
338.792937	17671.122597	29.089127
339.075511	17703.351232	29.094144
339.632810	17734.226317	29.099162
339.691081	17766.660782	29.104180
339.894079	17791.813068	29.109197
340.631495	17825.533530	29.114215
340.981088	17857.191848	29.119232
341.760268	17878.445731	29.124250
341.983673	17909.748286	29.129268
341.946465	17943.702564	29.134285
342.960879	17947.565302	29.139303
342.982415	17975.430538	29.144320
343.398567	17998.273466	29.149338
343.483792	18016.552808	29.154356
343.944135	18037.624714	29.159373
344.419424	18056.823216	29.164391
344.516880	18067.274710	29.169408
344.733670	18078.091093	29.174426
344.787252	18122.745837	29.179444
345.327975	18144.416173	29.184461
345.993311	18169.959218	29.189479
346.122579	18199.315478	29.194496
346.794012	18210.991542	29.199514
346.550772	18253.239915	29.204532
346.925305	18272.854100	29.209549
347.252481	18297.118138	29.214567
347.304043	18334.132208	29.219584
348.075539	18359.725788	29.224602
348.001557	18400.349844	29.229620
348.059486	18421.485567	29.234637
348.981805	18463.649111	29.239655
349.195201	18500.226993	29.244672
349.780641	18535.170390	29.249690
349.835637	18559.952656	29.254708
350.484870	18590.271923	29.259725
351.144912	18617.637119	29.264743
351.028618	18653.986078	29.269760
351.309841	18681.905756	29.274778
351.915842	18721.816131	29.279796
352.228724	18751.458293	29.284813
352.795072	18779.717221	29.289831
352.844279	18809.757709	29.294848
353.512852	18840.829281	29.299866
353.591832	18875.130396	29.304884
353.558809	18906.417301	29.309901
353.757974	18942.676947	29.314919
354.224977	18986.778648	29.319936
354.849784	19021.379242	29.324954
354.841263	19061.078269	29.329972
355.410043	19100.365184	29.334989
356.170297	19138.737826	29.340007
356.366089	19165.734525	29.345024
356.827405	19192.739423	29.350042
357.027734	19220.213087	29.355060
357.723842	19257.844696	29.360077
357.562714	19299.327106	29.365095
357.665313	19338.746769	29.370112
358.644737	19358.385269	29.375130
359.345462	19404.051025	29.380148
359.627993	19431.769979	29.385165
360.426860	19464.875172	29.390183
360.797212	19491.192534	29.395200
361.456683	19492.804938	29.400218
361.686401	19527.687817	29.405236
361.990588	19542.732680	29.410253
362.814428	19570.133871	29.415271
362.737939	19586.587867	29.420288
362.935876	19611.146315	29.425306
363.039481	19632.752096	29.430324
363.054915	19656.128538	29.435341
363.661630	19691.830669	29.440359
363.614768	19730.503533	29.445376
364.183781	19761.017905	29.450394
364.243129	19786.086604	29.455412
364.792599	19820.329287	29.460429
364.979015	19849.565528	29.465447
365.043279	19893.710948	29.470464
365.667593	19934.396799	29.475482
366.164151	19973.238983	29.480500
366.116260	20004.840958	29.485517
366.925540	20038.516231	29.490535
366.833486	20078.551494	29.495552
367.616455	20104.000852	29.500570
367.983436	20139.127173	29.505588
368.338813	20163.874819	29.510605
368.654608	20206.410987	29.515623
369.045812	20239.514131	29.520640
369.424606	20253.390223	29.525658
369.662662	20298.669826	29.530676
370.076495	20323.374947	29.535693
370.559570	20353.745385	29.540711
370.765253	20394.066422	29.545728
371.101228	20430.644069	29.550746
371.758755	20465.945359	29.555764
371.698738	20495.305417	29.560781
372.479412	20529.222876	29.565799
372.734724	20564.182520	29.570816
373.426732	20594.069593	29.575834
373.959855	20623.248340	29.580852
374.205753	20653.141427	29.585869
375.060112	20690.004475	29.590887
374.773368	20709.905771	29.595904
375.377841	20735.491206	29.600922
375.819456	20771.815679	29.605940
375.755918	20802.036032	29.610957
376.291604	20834.854797	29.615975
376.313955	20868.527748	29.620992
376.990782	20902.105261	29.626010
377.281445	20934.170152	29.631028
377.574178	20973.325799	29.636045
378.240860	21011.735565	29.641063
378.108373	21053.100940	29.646080
378.942666	21081.729412	29.651098
379.373931	21116.814066	29.656116
379.381650	21154.921552	29.661133
379.869365	21188.371655	29.666151
380.295731	21246.543775	29.671168
380.935932	21272.838293	29.676186
380.825784	21326.856920	29.681204
381.207856	21371.125582	29.686221
381.874619	21394.254972	29.691239
381.734405	21450.041519	29.696256
382.745585	21479.954704	29.701274
383.584827	21517.421161	29.706292
383.784623	21542.240695	29.711309
384.378973	21567.234722	29.716327
384.616485	21611.617764	29.721344
384.888058	21632.996586	29.726362
385.727518	21668.711801	29.731380
385.861785	21701.893395	29.736397
386.302910	21728.938850	29.741415
386.281099	21768.004848	29.746432
386.698742	21791.319409	29.751450
387.251694	21827.116975	29.756468
387.407924	21866.815949	29.761485
387.944436	21902.277429	29.766503
387.911022	21936.072095	29.771520
388.344431	21989.839097	29.776538
388.873526	22015.768452	29.781556
389.003703	22061.545195	29.786573
389.471788	22098.733722	29.791591
389.919020	22132.364247	29.796608
390.201019	22168.484782	29.801626
390.670421	22203.365183	29.806644
391.073848	22253.350983	29.811661
391.507398	22296.210402	29.816679
391.830897	22331.942893	29.821696
392.183761	22365.214238	29.826714
392.869416	22403.737581	29.831732
393.222975	22441.552785	29.836749
393.971657	22468.168659	29.841767
393.951730	22499.105378	29.846784
394.383234	22521.745444	29.851802
395.028488	22561.087787	29.856820
395.074549	22599.438169	29.861837
395.718437	22615.761947	29.866855
396.084932	22657.799322	29.871872
396.375499	22685.430898	29.876890
396.850992	22715.584567	29.881908
397.250646	22758.526443	29.886925
397.963030	22778.958863	29.891943
398.346511	22803.738881	29.896960
398.273524	22847.466980	29.901978
398.932797	22874.382067	29.906996
399.080896	22916.191284	29.912013
399.603236	22946.816937	29.917031
399.955620	22988.513753	29.922048
400.037666	23025.083822	29.927066
400.586476	23055.883465	29.932084
400.906249	23106.399614	29.937101
401.238107	23153.629671	29.942119
401.568915	23202.611741	29.947136
401.936770	23229.345338	29.952154
402.557266	23269.166435	29.957172
402.814764	23317.993820	29.962189
403.335580	23355.581627	29.967207
404.084876	23387.733110	29.972224
404.561892	23422.966387	29.977242
404.878503	23458.948372	29.982260
405.463590	23493.623130	29.987277
406.055466	23531.119177	29.992295
406.228631	23560.055035	29.997312
406.388851	23603.648808	30.002330
407.053864	23634.384587	30.007348
407.471180	23682.092368	30.012365
407.715684	23716.576296	30.017383
408.172371	23745.869283	30.022400
408.091347	23797.615768	30.027418
408.633082	23827.989113	30.032436
409.416236	23876.963060	30.037453
409.604132	23912.194661	30.042471
409.987795	23955.921143	30.047488
410.509057	24008.372930	30.052506
411.211078	24028.453807	30.057524
411.303881	24066.318879	30.062541
411.913477	24111.523723	30.067559
412.478260	24132.727988	30.072576
413.238511	24196.295039	30.077594
413.416453	24219.603678	30.082612
413.336009	24246.493355	30.087629
413.980533	24288.818410	30.092647
414.890414	24322.917719	30.097664
415.130021	24359.086210	30.102682
415.122320	24398.512315	30.107700
415.808611	24427.751210	30.112717
415.806709	24465.902451	30.117735
416.254430	24507.696063	30.122752
416.142121	24554.415245	30.127770
417.043432	24593.847750	30.132788
417.552800	24642.140645	30.137805
418.033424	24679.961943	30.142823
418.716421	24708.936959	30.147840
418.961824	24759.189645	30.152858
419.353374	24789.882817	30.157876
419.749247	24848.073970	30.162893
420.025613	24877.469659	30.167911
420.480346	24900.985807	30.172928
420.942969	24957.624145	30.177946
421.597266	24980.073018	30.182964
421.937641	25029.014634	30.187981
422.014111	25041.288918	30.192999
422.353675	25080.271329	30.198016
422.798764	25130.077408	30.203034
423.485712	25156.933217	30.208052
424.051797	25195.088458	30.213069
424.392875	25229.865422	30.218087
424.699414	25268.383808	30.223104
425.101524	25307.075721	30.228122
425.722328	25336.180349	30.233140
426.064675	25378.791417	30.238157
426.572929	25411.393402	30.243175
427.027717	25448.602533	30.248192
427.386770	25484.607033	30.253210
428.192145	25514.121433	30.258228
428.897269	25546.880387	30.263245
428.807272	25582.003661	30.268263
429.512427	25620.633612	30.273280
429.421298	25656.031608	30.278298
429.817544	25685.565005	30.283316
430.469935	25726.780610	30.288333
430.981926	25770.526831	30.293351
431.102987	25798.047981	30.298368
431.309904	25844.464077	30.303386
431.983091	25889.986420	30.308404
432.151298	25939.427441	30.313421
432.489385	25992.032298	30.318439
432.857922	26027.752525	30.323456
432.774960	26091.696181	30.328474
433.413546	26137.543446	30.333492
433.897334	26195.423473	30.338509
434.425147	26237.274331	30.343527
434.616633	26293.171826	30.348544
435.102561	26357.085579	30.353562
435.606085	26401.375720	30.358580
436.252262	26460.037236	30.363597
436.456492	26501.264082	30.368615
436.999983	26571.007183	30.373632
437.648174	26616.235958	30.378650
438.201483	26669.990104	30.383668
438.913530	26720.144668	30.388685
439.164469	26766.057651	30.393703
439.888527	26813.844967	30.398720
440.316989	26860.148367	30.403738
440.670818	26899.799658	30.408756
441.240480	26937.746879	30.413773
441.696163	26989.490079	30.418791
442.338050	27022.558794	30.423808
442.873907	27077.843686	30.428826
443.102224	27103.051446	30.433844
443.661010	27150.135246	30.438861
444.237295	27192.450395	30.443879
444.681576	27229.832306	30.448896
445.006159	27268.088842	30.453914
445.217039	27310.609732	30.458932
445.831917	27343.538438	30.463949
446.310265	27392.295275	30.468967
446.833578	27440.388755	30.473984
447.376779	27486.807367	30.479002
447.785151	27517.540511	30.484020
448.045342	27549.140356	30.489037
448.114250	27598.151507	30.494055
449.353864	27633.816356	30.499072
449.461664	27684.010465	30.504090
449.729665	27711.934654	30.509108
449.984477	27762.558915	30.514125
450.630132	27796.524302	30.519143
450.999516	27844.458238	30.524160
451.629329	27888.043728	30.529178
451.798998	27924.116179	30.534196
452.145159	27958.320613	30.539213
452.235098	28004.566305	30.544231
452.773123	28047.665831	30.549248
453.123099	28102.631439	30.554266
453.596982	28158.188690	30.559284
454.394366	28203.851222	30.564301
454.579948	28257.384030	30.569319
454.878968	28299.233546	30.574336
455.414141	28344.750503	30.579354
456.096884	28394.498420	30.584372
456.292453	28449.370772	30.589389
456.698385	28502.382170	30.594407
457.730376	28552.322048	30.599424
457.598760	28600.284059	30.604442
458.161544	28646.986456	30.609460
458.628259	28703.357324	30.614477
459.099352	28761.408955	30.619495
459.481784	28811.027876	30.624512
460.167148	28868.662788	30.629530
460.781887	28910.363844	30.634548
461.487394	28951.557913	30.639565
461.620011	29011.811321	30.644583
462.500056	29053.800117	30.649600
462.669795	29110.410634	30.654618
463.274905	29144.013143	30.659636
463.858950	29195.145560	30.664653
464.207282	29249.285451	30.669671
464.502235	29296.368217	30.674688
465.023937	29347.956169	30.679706
465.361814	29398.754460	30.684724
465.579121	29443.093390	30.689741
466.072277	29508.200584	30.694759
466.628883	29556.956914	30.699776
466.928856	29620.743134	30.704794
467.283501	29679.397515	30.709812
467.835985	29741.599878	30.714829
468.429082	29803.347801	30.719847
468.948927	29853.612627	30.724864
469.300799	29914.558509	30.729882
469.873655	29967.969534	30.734900
470.460985	30018.321483	30.739917
470.765886	30081.689011	30.744935
471.373971	30138.331417	30.749952
471.823009	30194.527077	30.754970
472.127918	30243.336370	30.759988
472.710629	30310.293038	30.765005
472.856074	30363.599213	30.770023
473.859316	30426.240630	30.775040
474.095999	30488.570384	30.780058
474.460120	30534.973119	30.785076
475.255764	30595.425346	30.790093
476.021033	30644.825373	30.795111
476.471332	30694.173459	30.800128
477.358848	30741.118088	30.805146
477.730509	30785.062675	30.810164
478.345145	30815.032536	30.815181
478.998760	30871.811770	30.820199
479.740141	30901.309708	30.825216
480.252449	30941.306882	30.830234
480.810042	30980.489034	30.835252
481.425698	31009.411661	30.840269
481.643765	31058.073528	30.845287
481.857830	31092.971628	30.850304
482.259644	31129.141737	30.855322
482.420096	31176.516808	30.860340
483.016645	31200.180614	30.865357
483.189005	31249.020923	30.870375
483.548875	31288.785373	30.875392
483.944696	31333.244747	30.880410
484.582469	31387.198345	30.885428
485.068680	31429.664917	30.890445
485.092099	31481.593882	30.895463
485.732596	31531.588067	30.900480
486.374139	31587.996187	30.905498
486.486716	31635.800013	30.910516
487.374069	31690.912197	30.915533
487.739405	31746.236979	30.920551
488.180210	31793.551635	30.925568
488.981677	31842.248668	30.930586
489.370280	31896.226062	30.935604
490.068784	31936.232615	30.940621
490.374499	31990.435374	30.945639
490.800331	32038.860569	30.950656
491.484113	32089.189936	30.955674
491.772902	32149.532490	30.960692
492.338702	32195.691774	30.965709
492.705867	32247.304356	30.970727
493.429611	32301.700895	30.975744
493.738923	32345.666005	30.980762
494.459430	32409.932453	30.985780
494.858948	32458.587161	30.990797
495.363528	32516.446986	30.995815
495.667857	32572.604771	31.000832
496.019306	32629.811915	31.005850
496.202306	32681.746461	31.010868
496.814477	32743.545784	31.015885
497.047483	32809.266697	31.020903
497.932677	32871.579834	31.025920
498.066287	32936.945331	31.030938
499.018118	33008.003538	31.035956
499.703291	33071.473665	31.040973
499.890687	33126.349433	31.045991
500.428242	33172.812534	31.051008
500.685901	33241.809248	31.056026
501.085201	33306.652634	31.061044
501.645418	33370.119232	31.066061
502.341292	33445.219175	31.071079
502.824277	33508.970382	31.076096
503.708367	33567.887935	31.081114
503.801255	33622.837649	31.086132
504.822266	33682.528103	31.091149
505.255784	33743.678892	31.096167
505.999538	33805.109958	31.101184
506.842213	33856.598220	31.106202
506.973890	33900.438777	31.111220
507.568958	33959.430618	31.116237
508.077662	34012.545862	31.121255
508.519129	34070.623146	31.126272
509.362318	34125.352672	31.131290
509.465067	34184.398181	31.136308
509.997166	34238.059274	31.141325
510.308383	34292.145130	31.146343
510.654492	34362.453716	31.151360
511.303386	34419.077940	31.156378
511.456548	34490.665299	31.161396
512.118009	34543.927296	31.166413
512.420397	34618.753263	31.171431
512.888984	34672.063280	31.176448
513.571285	34734.220854	31.181466
513.882583	34811.065670	31.186484
514.851290	34865.180356	31.191501
515.309991	34934.759462	31.196519
515.518410	34988.523618	31.201536
516.301851	35046.355120	31.206554
516.572211	35104.309424	31.211572
517.005040	35167.516339	31.216589
517.331171	35226.695655	31.221607
517.944457	35275.420618	31.226624
518.544024	35353.252034	31.231642
518.962229	35420.551917	31.236660
519.534172	35475.150534	31.241677
519.798474	35549.011611	31.246695
520.308755	35614.034427	31.251712
520.882787	35684.667173	31.256730
521.264841	35742.456784	31.261748
521.762086	35815.403211	31.266765
522.534539	35884.814284	31.271783
522.963540	35965.043308	31.276800
523.759944	36028.562437	31.281818
523.880732	36095.162925	31.286836
524.835670	36164.797402	31.291853
525.198263	36234.974950	31.296871
525.613589	36308.905736	31.301888
526.385442	36373.496795	31.306906
526.817157	36444.512650	31.311924
527.603739	36500.552701	31.316941
527.958296	36573.639395	31.321959
528.370987	36647.736115	31.326976
528.834317	36707.967494	31.331994
529.556712	36785.620751	31.337012
530.306932	36854.389150	31.342029
531.008872	36920.019382	31.347047
531.396917	36992.603621	31.352064
531.927437	37043.177485	31.357082
532.305352	37117.357628	31.362100
533.106841	37177.405336	31.367117
533.825757	37251.883174	31.372135
534.505430	37311.288705	31.377152
535.396580	37383.617848	31.382170
535.605837	37448.633920	31.387188
536.169789	37502.798201	31.392205
536.511984	37563.137666	31.397223
537.057957	37627.593810	31.402240
537.926972	37681.338990	31.407258
538.003011	37746.823138	31.412276
538.887984	37815.746538	31.417293
539.745842	37868.017097	31.422311
540.022415	37924.783349	31.427328
540.527846	37983.503454	31.432346
541.345649	38056.327135	31.437364
541.897432	38103.848546	31.442381
542.214916	38162.139486	31.447399
542.998543	38223.733808	31.452416
543.665020	38270.242541	31.457434
544.068461	38332.666963	31.462452
544.309464	38385.435422	31.467469
544.740185	38443.961058	31.472487
545.005308	38523.849824	31.477504
545.450475	38591.043507	31.482522
545.903976	38654.571742	31.487540
546.347620	38727.276867	31.492557
547.119891	38799.391451	31.497575
547.314866	38870.238189	31.502592
548.119095	38945.927225	31.507610
548.806268	39016.459678	31.512628
549.651420	39083.585967	31.517645
549.995557	39146.310207	31.522663
550.220628	39221.313298	31.527680
550.964041	39293.990120	31.532698
551.394002	39353.857086	31.537716
551.889824	39423.996628	31.542733
552.509922	39479.246484	31.547751
552.954954	39545.559955	31.552768
553.420214	39609.222156	31.557786
554.064501	39678.381785	31.562804
554.648498	39749.631682	31.567821
555.208238	39810.444564	31.572839
555.555503	39886.206682	31.577856
556.033233	39952.743496	31.582874
556.671770	40015.595711	31.587892
556.990417	40096.009668	31.592909
557.970634	40151.650300	31.597927
558.306690	40239.605899	31.602944
559.084552	40300.782105	31.607962
559.556921	40376.099473	31.612980
560.026457	40455.230658	31.617997
560.986143	40520.089599	31.623015
561.250281	40591.761771	31.628032
562.242501	40651.331805	31.633050
562.838950	40728.719751	31.638068
563.081548	40792.078795	31.643085
564.216074	40857.465611	31.648103
564.834768	40914.759189	31.653120
565.800129	40966.904130	31.658138
566.263601	41029.817162	31.663156
566.630073	41095.555803	31.668173
567.493614	41152.566628	31.673191
567.809639	41210.753938	31.678208
568.291877	41268.440486	31.683226
568.860166	41329.815741	31.688244
569.402295	41405.873951	31.693261
569.976895	41465.692388	31.698279
570.289622	41534.004689	31.703296
570.964352	41598.905053	31.708314
571.385971	41664.620843	31.713332
571.869975	41738.366702	31.718349
572.888124	41794.912051	31.723367
573.152841	41871.658823	31.728384
574.145958	41937.505326	31.733402
574.897742	42004.556768	31.738420
574.782930	42074.946233	31.743437
575.537345	42138.335878	31.748455
575.741428	42213.686167	31.753472
576.207278	42292.721716	31.758490
576.872387	42353.519331	31.763508
577.388612	42442.311233	31.768525
577.880588	42515.048702	31.773543
577.989342	42598.368396	31.778560
578.880400	42673.780729	31.783578
579.495345	42759.883986	31.788596
580.027690	42838.345808	31.793613
580.935813	42919.119896	31.798631
581.553959	42992.387710	31.803648
582.028045	43067.292802	31.808666
582.358173	43153.119768	31.813684
582.828118	43233.503529	31.818701
583.582102	43316.167420	31.823719
584.008014	43389.992618	31.828736
585.105145	43466.829527	31.833754
586.131081	43537.948528	31.838772
586.543181	43617.352206	31.843789
587.218650	43687.323679	31.848807
587.739475	43763.761349	31.853824
588.227732	43843.626976	31.858842
588.494269	43910.143540	31.863860
589.348880	43983.909769	31.868877
589.619942	44056.692941	31.873895
590.168145	44145.105721	31.878912
590.931540	44206.044737	31.883930
591.625001	44274.386372	31.888948
591.931721	44345.952445	31.893965
592.489702	44418.762261	31.898983
592.991438	44489.589471	31.904000
593.463944	44569.186142	31.909018
594.123466	44649.604711	31.914036
594.278796	44727.022297	31.919053
595.360330	44796.561487	31.924071
595.546929	44874.928005	31.929088
596.190945	44966.214581	31.934106
597.226427	45047.463121	31.939124
597.388382	45129.730855	31.944141
598.314859	45202.375524	31.949159
598.524548	45297.129548	31.954176
599.561061	45383.241646	31.959194
600.160999	45450.769508	31.964212
600.833851	45542.240420	31.969229
601.529492	45616.629798	31.974247
601.910581	45698.121858	31.979264
602.535848	45776.413390	31.984282
603.367757	45856.852891	31.989300
603.898498	45951.159367	31.994317
604.354454	46019.559250	31.999335
604.893564	46114.152491	32.004352
605.467321	46197.057854	32.009370
606.047240	46272.870866	32.014388
606.800219	46370.196026	32.019405
607.399801	46451.749999	32.024423
608.017553	46531.861494	32.029440
608.560822	46610.252145	32.034458
609.477176	46703.617760	32.039476
609.810002	46787.377011	32.044493
610.460838	46862.025018	32.049511
611.104031	46960.097607	32.054528
611.537981	47043.471856	32.059546
612.607579	47120.236791	32.064564
613.327848	47211.003853	32.069581
614.217885	47280.435489	32.074599
614.797307	47365.375434	32.079616
615.339877	47447.423100	32.084634
616.334307	47524.814687	32.089652
616.747814	47594.057777	32.094669
617.518017	47675.449930	32.099687
618.164687	47747.178087	32.104704
619.038672	47818.407944	32.109722
619.326953	47894.957721	32.114740
619.958490	47971.062712	32.119757
620.395972	48058.886993	32.124775
620.847824	48139.986367	32.129792
621.331142	48219.981975	32.134810
621.927381	48291.486846	32.139828
622.335889	48381.932081	32.144845
622.974443	48470.628201	32.149863
623.436276	48553.101357	32.154880
624.006174	48650.285354	32.159898
624.611848	48739.679736	32.164916
624.818543	48831.515178	32.169933
625.863203	48918.197889	32.174951
626.592951	49018.546870	32.179968
627.022783	49107.432015	32.184986
627.807674	49189.055613	32.190004
627.964630	49286.162634	32.195021
628.554943	49382.371183	32.200039
629.242955	49489.320280	32.205056
629.874038	49594.024544	32.210074
630.682829	49672.750351	32.215092
630.975914	49767.506701	32.220109
632.139037	49865.063158	32.225127
632.509812	49957.827506	32.230144
632.943517	50052.236760	32.235162
633.857977	50123.250664	32.240180
634.255223	50219.128972	32.245197
634.817375	50298.185481	32.250215
635.868759	50391.591166	32.255232
636.730444	50481.292511	32.260250
637.353882	50572.982229	32.265268
637.585263	50670.500868	32.270285
638.679777	50752.045271	32.275303
639.156594	50838.460974	32.280320
639.657049	50920.274747	32.285338
640.426234	51009.150585	32.290356
641.424729	51095.999247	32.295373
641.673606	51189.108670	32.300391
642.407482	51283.480727	32.305408
642.972555	51367.442859	32.310426
643.531633	51457.290333	32.315444
644.213486	51551.590180	32.320461
645.394755	51637.492021	32.325479
645.981282	51720.337245	32.330496
646.671039	51804.438609	32.335514
647.573432	51894.499887	32.340532
647.799952	51985.488081	32.345549
648.619305	52076.047160	32.350567
649.189254	52160.340418	32.355584
649.162763	52261.409267	32.360602
650.223411	52349.892566	32.365620
651.074797	52441.878864	32.370637
652.005180	52530.548746	32.375655
652.539953	52617.256594	32.380672
653.013608	52713.974875	32.385690
653.760036	52795.658066	32.390708
654.593585	52894.850977	32.395725
655.163297	52990.424004	32.400743
655.684308	53079.593576	32.405760
656.558554	53167.883980	32.410778
657.367526	53255.035824	32.415796
657.883881	53345.508743	32.420813
658.566060	53437.173942	32.425831
659.256740	53520.606657	32.430848
659.673757	53618.652807	32.435866
660.393385	53700.653785	32.440884
661.173051	53794.300868	32.445901
661.913877	53900.381286	32.450919
662.553803	53989.661742	32.455936
662.916543	54084.800515	32.460954
663.615971	54176.940163	32.465972
664.161640	54278.259835	32.470989
664.871736	54365.129734	32.476007
665.780589	54449.730745	32.481024
666.244714	54555.512951	32.486042
667.288675	54637.123149	32.491060
667.702499	54743.887608	32.496077
668.461492	54835.458245	32.501095
669.362443	54928.863302	32.506112
669.930961	55035.458494	32.511130
670.773939	55114.418793	32.516148
671.100609	55214.774942	32.521165
671.967377	55289.878101	32.526183
672.713399	55388.327366	32.531200
673.042996	55482.334855	32.536218
674.154826	55578.210103	32.541236
674.610957	55667.010487	32.546253
674.846158	55764.768880	32.551271
675.993569	55853.980346	32.556288
676.467196	55947.018554	32.561306
677.157324	56034.455144	32.566324
677.591389	56119.400817	32.571341
677.843662	56219.799652	32.576359
678.512022	56311.891280	32.581376
679.131197	56425.517856	32.586394
679.606641	56521.262700	32.591412
680.232523	56616.730430	32.596429
681.003048	56724.065928	32.601447
681.401359	56831.343428	32.606464
682.054520	56950.811949	32.611482
682.501816	57048.074103	32.616500
683.540172	57176.610588	32.621517
684.083938	57283.171477	32.626535
684.911240	57382.963129	32.631552
685.212154	57503.023913	32.636570
686.171801	57615.078300	32.641588
686.775093	57743.216407	32.646605
687.021911	57859.111610	32.651623
687.954281	57978.571803	32.656640
688.897560	58095.440197	32.661658
689.905533	58202.674977	32.666676
690.377367	58318.194474	32.671693
691.207028	58435.279512	32.676711
691.938710	58544.078301	32.681728
692.988651	58662.689080	32.686746
694.123130	58769.141419	32.691764
694.598445	58867.880180	32.696781
695.294550	58979.853071	32.701799
696.647444	59079.629623	32.706816
696.918893	59189.778080	32.711834
698.110940	59291.509599	32.716852
698.339466	59400.250801	32.721869
698.826627	59503.799680	32.726887
699.946133	59593.455964	32.731904
700.410969	59713.224922	32.736922
701.038496	59807.298471	32.741940
701.796892	59917.806545	32.746957
702.400476	60028.151211	32.751975
703.269455	60145.650526	32.756992
703.692632	60251.539389	32.762010
704.991747	60341.643318	32.767028
705.990953	60447.754065	32.772045
706.868999	60543.862505	32.777063
707.636404	60647.491068	32.782080
708.249988	60749.445578	32.787098
708.958416	60837.563789	32.792116
709.349886	60938.197201	32.797133
710.069795	61042.233777	32.802151
710.835627	61143.147653	32.807168
711.545315	61240.582771	32.812186
712.357874	61347.411613	32.817204
713.197661	61452.384799	32.822221
713.356947	61547.580255	32.827239
714.212483	61652.880515	32.832256
714.939037	61761.937726	32.837274
715.266006	61860.563983	32.842292
716.096542	61974.294606	32.847309
716.143231	62099.341843	32.852327
717.244230	62205.223802	32.857344
718.006874	62329.440049	32.862362
718.929626	62433.823159	32.867380
719.525117	62547.892856	32.872397
719.987260	62671.042134	32.877415
720.960939	62780.752908	32.882432
721.650724	62893.367941	32.887450
722.125629	63009.362550	32.892468
723.059127	63117.520644	32.897485
723.429299	63227.105947	32.902503
724.464600	63324.996600	32.907520
725.118648	63452.227196	32.912538
725.995295	63553.829994	32.917556
726.779121	63660.435546	32.922573
727.131845	63761.721380	32.927591
728.398002	63864.588722	32.932608
728.845030	63974.013637	32.937626
729.567030	64077.268978	32.942644
730.525623	64187.672429	32.947661
731.113078	64292.531253	32.952679
731.781465	64393.439398	32.957696
732.208700	64516.213651	32.962714
733.100270	64627.938946	32.967732
733.769549	64738.399452	32.972749
734.199875	64855.378961	32.977767
735.350788	64966.551271	32.982784
736.053370	65098.316178	32.987802
736.508080	65205.748937	32.992820
737.488889	65330.124338	32.997837
737.804968	65450.621639	33.002855
738.554957	65575.599212	33.007872
738.819388	65704.526290	33.012890
739.736005	65828.011356	33.017908
740.558613	65967.739369	33.022925
741.587887	66095.442675	33.027943
742.721426	66215.246835	33.032960
743.240370	66334.457827	33.037978
743.934819	66465.632247	33.042996
744.890924	66585.872418	33.048013
745.960203	66702.978100	33.053031
747.227503	66814.602587	33.058048
747.945211	66930.907882	33.063066
748.409811	67053.684686	33.068084
749.110299	67152.843578	33.073101
749.748969	67286.251272	33.078119
750.225546	67400.019762	33.083136
751.600359	67532.675297	33.088154
752.148199	67645.952905	33.093172
752.856999	67765.861415	33.098189
753.412006	67887.989689	33.103207
754.142098	68011.044367	33.108224
754.494357	68143.575506	33.113242
755.405141	68267.398413	33.118260
756.286228	68392.978150	33.123277
756.834796	68520.238312	33.128295
757.808925	68648.535333	33.133312
758.550868	68781.379149	33.138330
759.227521	68904.232934	33.143348
759.828154	69035.755071	33.148365
760.674210	69163.678084	33.153383
761.666648	69300.473138	33.158400
762.280490	69429.618376	33.163418
762.956253	69566.340999	33.168436
763.894797	69681.822139	33.173453
764.153882	69825.980831	33.178471
765.198183	69948.305801	33.183488
765.778203	70089.315280	33.188506
766.599267	70215.592290	33.193524
768.174353	70322.151861	33.198541
769.282566	70446.037152	33.203559
770.584137	70558.415626	33.208576
771.265572	70684.522484	33.213594
771.654828	70792.146443	33.218612
772.423697	70900.802097	33.223629
773.309036	71027.142871	33.228647
773.781137	71143.493020	33.233664
774.733925	71252.714445	33.238682
775.453529	71363.789603	33.243700
776.359735	71472.159932	33.248717
777.109341	71586.329526	33.253735
777.859068	71690.389257	33.258752
778.625939	71780.333699	33.263770
779.007265	71904.651012	33.268788
780.018188	72004.015376	33.273805
780.388600	72120.684825	33.278823
781.307864	72223.732749	33.283840
782.367474	72336.660084	33.288858
782.593430	72455.302745	33.293876
783.708408	72575.987100	33.298893
784.145955	72693.160759	33.303911
784.465255	72813.598442	33.308928
785.284097	72953.012897	33.313946
785.873890	73079.503118	33.318964
786.909734	73216.474233	33.323981
787.190122	73354.386695	33.328999
787.906074	73497.685307	33.334016
788.447958	73628.214737	33.339034
789.368406	73772.961120	33.344052
789.880706	73924.131126	33.349069
790.771016	74069.377713	33.354087
791.794639	74218.511323	33.359104
792.747865	74362.010459	33.364122
793.441909	74503.940771	33.369140
794.669469	74650.912557	33.374157
795.149985	74802.688378	33.379175
796.120507	74947.731560	33.384192
797.532518	75075.615420	33.389210
798.177408	75226.848492	33.394228
798.860333	75361.874087	33.399245
799.651498	75506.659703	33.404263
800.497830	75647.174698	33.409280
801.657128	75780.062551	33.414298
802.576933	75923.507935	33.419316
803.559906	76057.931758	33.424333
804.417423	76181.372846	33.429351
804.988843	76323.487035	33.434368
805.702259	76449.615974	33.439386
806.499204	76597.879938	33.444404
807.382339	76722.749162	33.449421
808.072457	76868.173939	33.454439
808.765793	77001.196736	33.459456
809.785220	77140.377219	33.464474
810.350513	77283.156381	33.469492
811.543197	77418.452000	33.474509
811.967457	77570.155093	33.479527
812.486358	77705.848344	33.484544
813.388340	77841.472847	33.489562
813.845868	78002.546728	33.494580
814.773674	78145.524597	33.499597
815.664379	78299.059449	33.504615
816.414227	78452.751449	33.509632
817.589742	78596.829817	33.514650
817.926546	78746.316361	33.519668
819.058938	78894.059646	33.524685
819.906167	79042.844044	33.529703
820.422416	79185.966147	33.534720
821.947184	79338.366159	33.539738
822.528929	79479.689303	33.544756
823.852025	79620.726471	33.549773
824.317549	79765.574820	33.554791
825.203896	79915.067014	33.559808
826.133752	80044.634336	33.564826
826.823679	80200.745612	33.569844
828.141210	80329.921649	33.574861
828.806685	80469.573621	33.579879
829.392713	80608.138933	33.584896
830.386918	80734.473585	33.589914
831.379736	80863.080077	33.594932
832.514896	80986.596944	33.599949
833.149462	81111.576152	33.604967
833.941562	81234.081981	33.609984
834.863033	81349.355743	33.615002
835.185932	81496.263051	33.620020
836.295977	81619.895079	33.625037
837.182775	81747.821960	33.630055
837.688074	81885.200216	33.635072
838.823683	82018.205210	33.640090
839.508347	82160.110204	33.645108
840.519329	82286.128154	33.650125
841.057629	82417.595681	33.655143
842.385681	82553.614881	33.660160
843.239812	82673.239891	33.665178
843.829783	82825.634438	33.670196
844.716134	82958.154705	33.675213
845.473684	83091.917979	33.680231
846.274570	83239.516805	33.685248
847.163182	83368.312900	33.690266
847.554691	83517.891675	33.695284
848.642052	83652.154171	33.700301
849.567733	83809.908944	33.705319
850.168828	83957.671930	33.710336
850.836389	84095.283468	33.715354
851.588908	84251.785593	33.720372
852.576294	84407.592038	33.725389
853.487198	84566.619784	33.730407
854.722655	84696.454271	33.735424
855.854862	84839.940648	33.740442
856.567831	85003.515062	33.745460
857.624083	85138.854302	33.750477
858.478256	85286.438532	33.755495
858.759526	85434.807935	33.760512
859.628170	85583.397652	33.765530
860.256581	85741.448864	33.770548
861.105508	85901.653894	33.775565
862.014296	86051.309257	33.780583
862.328403	86218.058390	33.785600
863.477418	86377.521180	33.790618
864.151609	86552.147510	33.795636
865.195030	86715.185941	33.800653
866.098540	86880.811170	33.805671
866.816404	87056.927319	33.810688
868.142610	87204.989975	33.815706
869.012537	87365.828044	33.820724
870.043752	87531.145746	33.825741
870.805904	87700.938303	33.830759
871.535552	87855.469064	33.835776
872.632871	88013.705057	33.840794
873.291834	88179.816480	33.845812
874.484570	88329.028286	33.850829
875.293882	88496.730686	33.855847
875.973187	88657.526838	33.860864
877.318201	88824.744476	33.865882
877.870287	88990.284458	33.870900
879.087822	89142.053785	33.875917
879.731037	89295.924874	33.880935
880.842294	89448.125034	33.885952
881.857143	89611.036455	33.890970
882.612829	89761.310341	33.895988
883.130154	89915.832728	33.901005
884.629047	90082.198554	33.906023
884.921003	90252.144086	33.911040
886.113348	90398.806123	33.916058
886.851144	90559.067646	33.921076
887.484568	90711.639587	33.926093
888.787492	90864.962620	33.931111
889.642623	91022.841084	33.936128
890.714136	91156.421624	33.941146
891.413611	91307.853683	33.946164
891.977956	91454.828423	33.951181
893.091346	91599.530061	33.956199
894.034181	91757.943156	33.961216
894.765519	91906.171471	33.966234
895.542657	92062.841921	33.971252
896.209456	92216.848236	33.976269
897.130017	92374.895688	33.981287
897.928642	92537.426116	33.986304
898.806552	92708.811262	33.991322
899.517949	92867.491394	33.996340
900.487962	93037.135881	34.001357
901.168240	93213.240652	34.006375
901.607862	93387.728235	34.011392
902.824359	93559.728062	34.016410
903.546653	93733.753748	34.021428
904.322063	93924.942928	34.026445
905.401442	94097.912258	34.031463
906.250751	94288.655383	34.036480
907.502481	94464.086261	34.041498
908.308951	94650.655625	34.046516
908.941802	94822.925321	34.051533
909.909782	95013.224122	34.056551
910.682946	95210.436734	34.061568
912.006141	95384.906676	34.066586
912.937291	95561.537684	34.071604
913.688222	95760.157230	34.076621
914.781569	95946.302996	34.081639
915.772359	96135.612983	34.086656
916.822032	96320.775026	34.091674
917.738856	96505.371720	34.096692
918.488130	96691.871103	34.101709
919.323654	96879.091924	34.106727
920.132322	97068.850587	34.111744
921.129098	97253.078856	34.116762
921.921124	97458.288509	34.121780
922.549496	97655.000198	34.126797
923.643724	97832.620690	34.131815
924.701524	98039.069951	34.136832
925.371137	98236.893550	34.141850
926.375152	98440.113914	34.146868
927.345993	98631.794806	34.151885
928.519593	98831.439015	34.156903
929.582704	99022.683530	34.161920
930.826124	99209.651958	34.166938
932.106744	99385.169977	34.171956
933.513210	99571.189916	34.176973
935.031548	99744.233913	34.181991
936.236788	99920.166946	34.187008
936.914322	100078.493919	34.192026
937.964888	100251.555325	34.197044
939.253208	100417.424834	34.202061
940.205202	100560.502884	34.207079
940.893322	100733.849014	34.212096
941.946123	100901.083738	34.217114
942.981686	101056.762036	34.222132
943.658588	101235.260534	34.227149
944.771690	101380.437507	34.232167
945.760324	101537.171123	34.237184
946.229208	101701.398951	34.242202
947.475411	101868.006648	34.247220
948.591100	102030.236781	34.252237
949.526448	102189.806932	34.257255
949.793379	102359.833787	34.262272
950.929437	102524.665861	34.267290
951.889898	102676.200423	34.272308
952.547085	102845.184700	34.277325
953.733185	103005.193388	34.282343
954.196189	103168.431225	34.287360
954.925298	103313.138060	34.292378
955.992617	103491.568846	34.297396
956.759327	103651.568483	34.302413
957.840204	103831.689927	34.307431
958.568048	103989.969533	34.312448
959.390316	104170.699557	34.317466
960.309244	104336.655476	34.322484
960.997036	104517.068200	34.327501
962.333745	104699.502553	34.332519
963.055705	104887.903044	34.337536
963.840212	105069.513033	34.342554
964.823427	105256.631993	34.347572
965.710435	105457.211145	34.352589
966.840185	105633.715078	34.357607
967.421186	105828.509400	34.362624
968.045270	106044.637579	34.367642
969.246053	106238.167496	34.372660
970.101282	106422.143463	34.377677
971.826117	106626.924537	34.382695
972.816037	106821.532068	34.387712
973.774060	107014.436545	34.392730
974.600517	107211.492933	34.397748
975.665122	107400.595808	34.402765
977.002747	107598.609225	34.407783
977.838256	107795.212521	34.412800
978.969701	107989.425328	34.417818
979.969699	108169.640624	34.422836
981.194069	108350.200065	34.427853
983.714205	108507.482758	34.432871
985.171328	108676.290319	34.437888
986.141188	108849.701069	34.442906
987.287797	109007.479461	34.447924
987.871330	109165.047765	34.452941
989.381790	109315.421684	34.457959
989.986162	109499.739063	34.462976
990.784843	109658.820010	34.467994
991.502928	109812.418071	34.473012
992.164427	109982.859842	34.478029
993.378473	110153.629459	34.483047
993.761511	110335.899158	34.488064
994.492806	110507.042042	34.493082
995.559224	110693.140623	34.498100
996.352549	110880.919576	34.503117
997.696559	111066.658230	34.508135
998.403291	111267.108285	34.513152
999.179142	111454.438087	34.518170
1000.304263	111634.022613	34.523188
1001.413169	111829.926284	34.528205
1002.474266	112020.557018	34.533223
1003.159809	112214.329246	34.538240
1003.564861	112417.434373	34.543258
1004.709896	112612.539648	34.548276
1005.557224	112821.490483	34.553293
1006.345617	113019.317729	34.558311
1007.462558	113232.318846	34.563328
1008.047566	113451.718044	34.568346
1009.094224	113663.822014	34.573364
1010.218689	113872.595728	34.578381
1011.385338	114075.384673	34.583399
1012.221279	114296.839406	34.588416
1013.237915	114503.380727	34.593434
1014.404904	114719.248097	34.598452
1015.205072	114941.828707	34.603469
1016.446913	115139.608927	34.608487
1017.465915	115341.088610	34.613504
1017.938941	115562.169922	34.618522
1019.332633	115750.351743	34.623540
1020.003081	115961.914581	34.628557
1021.390506	116176.388572	34.633575
1022.595335	116373.854232	34.638592
1023.530588	116580.918448	34.643610
1025.076709	116764.698323	34.648628
1025.918891	116972.173532	34.653645
1027.381864	117158.427583	34.658663
1028.296740	117354.376952	34.663680
1029.284034	117552.203516	34.668698
1030.477390	117741.077873	34.673716
1031.481651	117945.632065	34.678733
1032.484598	118147.856661	34.683751
1033.581921	118348.458010	34.688768
1034.671071	118543.081785	34.693786
1035.657251	118740.017209	34.698804
1036.385467	118957.484572	34.703821
1037.857125	119154.165314	34.708839
1038.748547	119357.113756	34.713856
1039.256998	119565.321821	34.718874
1040.493757	119774.488170	34.723892
1041.640046	119990.690616	34.728909
1042.430133	120205.927141	34.733927
1043.513647	120419.064122	34.738944
1044.134522	120636.283121	34.743962
1045.783067	120852.307725	34.748980
1047.108323	121060.341030	34.753997
1048.028723	121274.917743	34.759015
1049.306427	121483.620838	34.764032
1050.097959	121702.834398	34.769050
1051.188189	121918.883058	34.774068
1051.839168	122134.676362	34.779085
1053.118599	122351.406599	34.784103
1054.238463	122579.962372	34.789120
1055.049836	122799.168183	34.794138
1056.147481	123016.478232	34.799156
1056.929741	123260.314272	34.804173
1057.965174	123488.460172	34.809191
1059.180669	123716.932933	34.814208
1060.172434	123950.044524	34.819226
1060.976229	124169.793990	34.824244
1061.961588	124421.057559	34.829261
1062.640107	124653.542045	34.834279
1063.830714	124894.510714	34.839296
1064.924937	125137.816406	34.844314
1065.972022	125380.979776	34.849332
1066.867589	125624.309536	34.854349
1068.109444	125868.091032	34.859367
1068.883790	126121.139939	34.864384
1070.108772	126365.637957	34.869402
1071.695545	126604.691918	34.874420
1072.425032	126858.413431	34.879437
1073.806793	127096.288430	34.884455
1075.141865	127337.354166	34.889472
1076.192026	127575.896007	34.894490
1077.832487	127820.615981	34.899508
1079.053140	128042.340045	34.904525
1080.442052	128272.605805	34.909543
1081.576040	128487.401847	34.914560
1082.428529	128724.895269	34.919578
1084.071477	128937.785304	34.924596
1085.082739	129164.583865	34.929613
1086.146705	129385.050655	34.934631
1087.161813	129602.193582	34.939648
1087.943499	129830.327761	34.944666
1089.469937	130032.927121	34.949684
1090.231944	130252.537319	34.954701
1091.003912	130463.160662	34.959719
1092.343256	130670.713059	34.964736
1093.398442	130884.182466	34.969754
1094.268109	131089.825136	34.974772
1095.484806	131302.751039	34.979789
1096.464249	131525.718666	34.984807
1097.653189	131732.491679	34.989824
1098.466281	131965.465715	34.994842
1099.469815	132181.981995	34.999860
1100.614215	132404.751143	35.004877
1101.424008	132629.909502	35.009895
1102.633937	132844.114535	35.014912
1103.532145	133088.871663	35.019930
1104.519182	133318.239526	35.024948
1105.527537	133567.330151	35.029965
1106.667338	133790.642175	35.034983
1107.472329	134033.165493	35.040000
1108.015200	134292.632069	35.045018
1109.308307	134539.743693	35.050036
1110.313870	134791.595164	35.055053
1111.201899	135047.119002	35.060071
1112.777725	135298.233754	35.065088
1113.857129	135564.264822	35.070106
1114.925931	135822.452515	35.075124
1115.968842	136087.695214	35.080141
1117.266761	136342.236119	35.085159
1118.493317	136589.653248	35.090176
1119.556525	136870.822127	35.095194
1120.749558	137126.438697	35.100212
1122.126645	137389.532242	35.105229
1123.177181	137644.428353	35.110247
1124.678230	137895.296468	35.115264
1126.278472	138147.532044	35.120282
1127.701779	138394.702038	35.125300
1128.740226	138645.183089	35.130317
1129.709223	138894.295524	35.135335
1131.244654	139140.133971	35.140352
1132.035363	139388.151117	35.145370
1133.301957	139633.302195	35.150388
1134.310019	139883.886290	35.155405
1135.182346	140139.845211	35.160423
1136.349224	140384.637851	35.165440
1137.427989	140653.207682	35.170458
1138.435330	140900.756426	35.175476
1139.662764	141155.155568	35.180493
1140.612194	141421.914313	35.185511
1141.864799	141674.893077	35.190528
1142.797610	141945.982409	35.195546
1144.228277	142195.423350	35.200564
1145.329976	142460.009489	35.205581
1146.360395	142734.740749	35.210599
1147.726363	142988.572725	35.215616
1148.533460	143261.607869	35.220634
1150.011863	143514.360008	35.225652
1151.230399	143777.580159	35.230669
1152.484466	144037.081056	35.235687
1153.991926	144289.466299	35.240704
1155.188581	144549.360900	35.245722
1156.379855	144802.410709	35.250740
1157.506764	145062.269902	35.255757
1158.499191	145312.008461	35.260775
1159.801952	145558.933097	35.265792
1161.252772	145818.325924	35.270810
1162.525951	146066.108621	35.275828
1163.971107	146306.585596	35.280845
1165.101409	146554.813770	35.285863
1166.646122	146783.395080	35.290880
1167.551682	147025.056581	35.295898
1168.683869	147246.784822	35.300916
1169.803674	147466.893221	35.305933
1170.685156	147694.562606	35.310951
1171.896885	147908.228867	35.315968
1173.135177	148144.618049	35.320986
1174.022311	148382.385672	35.326004
1175.378309	148620.090145	35.331021
1175.918254	148855.229569	35.336039
1177.287848	149099.504311	35.341056
1178.342223	149352.685012	35.346074
1179.587409	149596.222673	35.351092
1180.439049	149847.601309	35.356109
1181.024208	150103.084092	35.361127
1182.066001	150363.490264	35.366144
1183.087606	150632.893716	35.371162
1184.192437	150909.514648	35.376180
1185.435058	151184.643672	35.381197
1186.242829	151457.741119	35.386215
1187.443009	151739.463775	35.391232
1188.317414	152022.282359	35.396250
1189.308593	152316.498843	35.401268
1190.742910	152606.902861	35.406285
1191.838430	152914.031265	35.411303
1192.791103	153201.018691	35.416320
1194.134042	153498.382621	35.421338
1194.847391	153803.881696	35.426356
1196.169294	154103.676453	35.431373
1197.267164	154420.405739	35.436391
1198.656190	154716.756837	35.441408
1199.968512	155041.002939	35.446426
1201.017215	155346.902914	35.451444
1202.752711	155656.941252	35.456461
1203.522888	155959.619446	35.461479
1205.133668	156273.704313	35.466496
1206.831243	156568.509189	35.471514
1208.025527	156872.456369	35.476532
1209.518595	157171.726570	35.481549
1210.747455	157478.019453	35.486567
1212.866724	157773.093584	35.491584
1214.062751	158059.861234	35.496602
1215.549742	158353.014409	35.501620
1217.065075	158634.253426	35.506637
1218.155254	158912.215621	35.511655
1219.481338	159197.422359	35.516672
1220.706394	159478.448828	35.521690
1221.808354	159765.434536	35.526708
1223.344817	160044.802459	35.531725
1223.745383	160339.151659	35.536743
1225.436013	160613.410977	35.541760
1226.418668	160896.390217	35.546778
1227.499224	161195.314566	35.551796
1228.825181	161474.828546	35.556813
1230.282769	161772.286688	35.561831
1231.280489	162056.755766	35.566848
1232.494974	162348.739558	35.571866
1233.567251	162647.028797	35.576884
1234.974830	162923.215197	35.581901
1236.088799	163222.630807	35.586919
1237.254981	163513.641173	35.591936
1238.707901	163803.527834	35.596954
1239.687115	164099.102397	35.601972
1241.672210	164383.145252	35.606989
1242.232981	164685.669463	35.612007
1243.115067	164964.886786	35.617024
1244.419576	165263.790634	35.622042
1245.783839	165564.564475	35.627060
1247.356764	165855.688738	35.632077
1248.151308	166150.064636	35.637095
1249.677885	166418.743049	35.642112
1250.871001	166696.359709	35.647130
1251.535980	166984.786673	35.652148
1253.505797	167269.333328	35.657165
1254.419648	167544.806464	35.662183
1255.838169	167835.626937	35.667200
1257.009107	168122.303056	35.672218
1258.250701	168404.135098	35.677236
1259.840374	168689.819543	35.682253
1260.892524	168984.755700	35.687271
1262.614385	169259.332187	35.692288
1263.605893	169547.316014	35.697306
1264.416013	169840.584803	35.702324
1265.870582	170137.644635	35.707341
1266.989176	170420.804004	35.712359
1268.099968	170722.708179	35.717376
1269.351045	171017.041171	35.722394
1270.260278	171331.456097	35.727412
1271.624152	171646.026561	35.732429
1272.830106	171960.929798	35.737447
1273.771015	172273.391799	35.742464
1275.703986	172579.118978	35.747482
1277.103836	172896.915214	35.752500
1278.550302	173183.717568	35.757517
1280.347393	173493.851166	35.762535
1282.060395	173790.968166	35.767552
1283.102654	174093.844799	35.772570
1284.298181	174394.045860	35.777588
1285.544200	174695.344539	35.782605
1286.466044	175005.010741	35.787623
1287.694415	175318.816173	35.792640
1289.185728	175617.148745	35.797658
1290.158758	175950.391394	35.802676
1291.664519	176255.121553	35.807693
1292.463399	176580.960635	35.812711
1293.695437	176901.831794	35.817728
1294.612140	177222.351007	35.822746
1295.744035	177558.370473	35.827764
1297.121139	177873.817751	35.832781
1298.296640	178225.609482	35.837799
1299.487248	178564.012045	35.842816
1301.074987	178898.708982	35.847834
1301.943642	179245.659765	35.852852
1303.566091	179583.261879	35.857869
1304.779632	179924.842734	35.862887
1306.357369	180265.946970	35.867904
1308.031734	180600.272890	35.872922
1309.320397	180952.826578	35.877940
1310.837605	181274.288024	35.882957
1311.998730	181620.965652	35.887975
1313.333384	181962.083253	35.892992
1314.546142	182294.338753	35.898010
1315.455179	182644.948623	35.903028
1316.869815	182981.998217	35.908045
1318.085203	183329.046351	35.913063
1319.057668	183679.398818	35.918080
1320.442763	184041.895701	35.923098
1321.579942	184401.960914	35.928116
1323.147455	184754.354611	35.933133
1324.244092	185118.492991	35.938151
1325.480858	185465.246876	35.943168
1326.966171	185825.505321	35.948186
1327.879041	186192.029434	35.953204
1329.418739	186562.323947	35.958221
1330.856513	186924.146030	35.963239
1332.331738	187276.228561	35.968256
1333.573111	187628.618479	35.973274
1334.513556	187994.312231	35.978292
1335.973722	188343.230620	35.983309
1337.366918	188677.729610	35.988327
1338.965510	189036.809698	35.993344
1341.080486	189389.193386	35.998362
1341.969964	189727.615194	36.003380
1343.141598	190072.301294	36.008397
1344.526541	190414.834355	36.013415
1345.654005	190778.852182	36.018432
1346.749196	191129.320276	36.023450
1347.546882	191496.227784	36.028468
1348.819483	191867.121369	36.033485
1350.017939	192241.165020	36.038503
1350.918374	192621.569344	36.043520
1352.301482	192990.484044	36.048538
1354.021573	193384.455320	36.053556
1354.962760	193763.171741	36.058573
1356.879550	194151.999574	36.063591
1358.014305	194540.070298	36.068608
1359.659405	194911.505056	36.073626
1361.274526	195310.101599	36.078644
1362.542474	195687.849180	36.083661
1363.987695	196080.219995	36.088679
1365.099597	196471.899238	36.093696
1366.320515	196849.648837	36.098714
1367.873450	197254.272804	36.103732
1369.451127	197658.019247	36.108749
1371.031880	198048.208852	36.113767
1372.366919	198446.096810	36.118784
1373.657744	198831.400342	36.123802
1374.957425	199234.097879	36.128820
1376.579208	199616.253594	36.133837
1377.942145	200023.579454	36.138855
1379.141084	200431.963223	36.143872
1380.589502	200837.058086	36.148890
1381.679057	201238.761226	36.153908
1383.179440	201643.280962	36.158925
1384.569652	202053.052127	36.163943
1385.895994	202458.786100	36.168960
1387.396732	202875.184057	36.173978
1389.059605	203287.063143	36.178996
1390.085940	203687.711599	36.184013
1391.750818	204097.004927	36.189031
1393.181812	204509.094369	36.194048
1394.775819	204914.214091	36.199066
1396.360974	205317.293319	36.204084
1397.562105	205727.408756	36.209101
1399.077858	206133.525762	36.214119
1400.738217	206533.755053	36.219136
1402.434825	206950.182066	36.224154
1403.801916	207348.496007	36.229172
1405.216541	207757.965101	36.234189
1406.785602	208154.980166	36.239207
1407.977689	208563.829987	36.244224
1409.490134	208957.087345	36.249242
1410.981639	209370.920160	36.254260
1412.165731	209768.984623	36.259277
1413.575586	210172.549998	36.264295
1414.777995	210581.662445	36.269312
1416.473035	210981.235782	36.274330
1418.121901	211380.107604	36.279348
1419.204147	211784.077840	36.284365
1421.261193	212183.597245	36.289383
1422.398211	212589.111481	36.294400
1423.453493	212989.434915	36.299418
1425.005606	213397.017779	36.304436
1426.254645	213801.960558	36.309453
1428.130779	214199.589105	36.314471
1429.226684	214596.027581	36.319488
1430.893418	214970.481585	36.324506
1432.099196	215374.016505	36.329524
1433.303975	215755.838938	36.334541
1434.334809	216190.974882	36.339559
1435.784224	216621.599293	36.344576
1437.045789	217026.427570	36.349594
1438.221319	217419.741341	36.354612
1439.654255	217831.884684	36.359629
1441.298098	218240.617113	36.364647
1442.466784	218661.493652	36.369664
1444.030559	219061.988481	36.374682
1445.699158	219483.268630	36.379700
1446.544310	219904.203892	36.384717
1447.969192	220330.582073	36.389735
1449.333816	220760.883341	36.394752
1450.717385	221190.497537	36.399770
1452.161540	221622.617979	36.404788
1453.634219	222058.443706	36.409805
1455.216278	222507.943120	36.414823
1456.527049	222945.526321	36.419840
1457.964556	223384.360328	36.424858
1459.524202	223837.348627	36.429876
1460.662702	224275.143366	36.434893
1462.154667	224725.784323	36.439911
1463.389823	225177.383826	36.444928
1464.809088	225641.603665	36.449946
1466.442411	226106.120226	36.454964
1467.678837	226568.875334	36.459981
1468.885877	227041.238199	36.464999
1470.477786	227512.447199	36.470016
1471.841110	227985.118123	36.475034
1473.279803	228465.627025	36.480052
1474.352565	228945.055125	36.485069
1476.247787	229427.676730	36.490087
1477.834950	229910.401755	36.495104
1479.648958	230391.059070	36.500122
1481.486317	230877.810377	36.505140
1482.849203	231350.061748	36.510157
1484.425775	231816.310294	36.515175
1485.980498	232305.373900	36.520192
1487.634415	232780.960334	36.525210
1489.444837	233250.299253	36.530228
1491.151138	233726.362711	36.535245
1492.996685	234192.041031	36.540263
1494.319345	234661.642624	36.545280
1496.570495	235118.798196	36.550298
1498.147584	235563.213227	36.555316
1499.501762	236035.353798	36.560333
1501.281049	236492.184676	36.565351
1502.734090	236956.233865	36.570368
1504.423445	237405.486971	36.575386
1505.625971	237861.705417	36.580404
1506.424310	238331.124427	36.585421
1508.732598	238782.590424	36.590439
1509.983370	239240.734896	36.595456
1511.812154	239705.415000	36.600474
1513.652812	240149.366227	36.605492
1514.968060	240610.068891	36.610509
1516.463234	241057.559216	36.615527
1517.512036	241518.714316	36.620544
1519.005619	241978.298293	36.625562
1520.365999	242433.663039	36.630580
1522.503422	242897.130848	36.635597
1523.725148	243341.368682	36.640615
1525.216951	243800.702632	36.645632
1527.142629	244251.735465	36.650650
1528.839144	244697.040562	36.655668
1530.427124	245139.214429	36.660685
1532.189690	245556.922937	36.665703
1532.868256	245994.879040	36.670720
1534.270342	246430.582626	36.675738
1535.679267	246860.493928	36.680756
1536.668340	247310.568710	36.685773
1538.448001	247773.316710	36.690791
1539.733679	248222.658000	36.695808
1541.127417	248680.644451	36.700826
1542.279296	249149.112017	36.705844
1543.371850	249623.229443	36.710861
1545.025844	250092.656905	36.715879
1545.623452	250583.877190	36.720896
1547.292935	251079.468352	36.725914
1549.275327	251574.119356	36.730932
1550.503333	252068.031679	36.735949
1552.277731	252561.244689	36.740967
1553.527325	253056.424610	36.745984
1555.348239	253564.288506	36.751002
1557.260554	254067.133348	36.756020
1558.799254	254585.307568	36.761037
1560.439372	255083.752566	36.766055
1561.373657	255596.108322	36.771072
1562.646706	256106.350848	36.776090
1564.772659	256632.558603	36.781108
1566.517605	257148.464969	36.786125
1568.068512	257668.214076	36.791143
1570.024204	258183.501827	36.796160
1571.328243	258708.042451	36.801178
1573.129343	259227.090294	36.806196
1574.728052	259743.351863	36.811213
1576.231852	260260.391255	36.816231
1578.072600	260798.078779	36.821248
1579.339743	261318.180238	36.826266
1581.786509	261825.410775	36.831284
1583.557946	262339.840191	36.836301
1585.163332	262847.565027	36.841319
1586.768278	263370.353952	36.846336
1588.574545	263885.005836	36.851354
1590.214484	264387.389778	36.856372
1591.799213	264907.463269	36.861389
1593.561827	265424.103098	36.866407
1594.931958	265935.117057	36.871424
1596.361675	266455.647053	36.876442
1598.012717	266966.309118	36.881460
1599.297097	267488.183273	36.886477
1601.357852	267999.030930	36.891495
1602.878615	268525.310703	36.896512
1604.276972	269042.439627	36.901530
1606.056607	269558.336557	36.906548
1607.916268	270073.305199	36.911565
1609.795583	270594.696952	36.916583
1611.157255	271101.566746	36.921600
1612.609511	271634.839999	36.926618
1614.310272	272156.030516	36.931636
1615.826090	272677.784247	36.936653
1617.338974	273190.926108	36.941671
1619.310277	273728.937065	36.946688
1620.954642	274249.244528	36.951706
1622.457098	274760.150108	36.956724
1623.829840	275302.804103	36.961741
1625.703043	275822.893175	36.966759
1627.215073	276343.269462	36.971776
1628.610233	276870.040022	36.976794
1630.323314	277395.055069	36.981812
1631.844225	277930.109239	36.986829
1633.418542	278461.190628	36.991847
1635.180295	278984.974819	36.996864
1636.698652	279494.572702	37.001882
1638.626042	279992.518525	37.006900
1639.990301	280495.560300	37.011917
1641.719442	281008.777669	37.016935
1643.331847	281515.230665	37.021952
1644.761147	282032.508373	37.026970
1646.754255	282540.013568	37.031988
1648.230161	283053.368919	37.037005
1649.827567	283569.623977	37.042023
1651.366637	284090.256247	37.047040
1652.762000	284617.007046	37.052058
1654.675173	285134.297653	37.057076
1656.529053	285663.865309	37.062093
1657.817759	286189.511095	37.067111
1659.700989	286720.061109	37.072128
1661.134145	287257.059268	37.077146
1662.555614	287787.986637	37.082164
1664.039043	288330.408543	37.087181
1665.395373	288884.965633	37.092199
1666.969468	289431.026228	37.097216
1668.476913	289995.790600	37.102234
1670.397038	290551.873818	37.107252
1671.927413	291123.106941	37.112269
1673.459313	291686.742686	37.117287
1674.858212	292260.710455	37.122304
1676.260417	292836.783345	37.127322
1678.117098	293423.497441	37.132340
1679.806465	294015.214759	37.137357
1681.239605	294598.284786	37.142375
1683.354891	295178.293096	37.147392
1684.652431	295785.966530	37.152410
1686.902551	296369.655042	37.157428
1688.311122	296954.266795	37.162445
1690.057192	297554.592674	37.167463
1692.017155	298153.483075	37.172480
1693.728077	298754.468579	37.177498
1695.769345	299346.303497	37.182516
1697.529519	299932.085830	37.187533
1699.242336	300530.597273	37.192551
1700.987109	301138.903672	37.197568
1702.874720	301726.508807	37.202586
1704.932017	302311.923658	37.207604
1706.274514	302904.767504	37.212621
1708.275133	303516.775942	37.217639
1710.438531	304092.028875	37.222656
1711.887557	304687.485416	37.227674
1713.980341	305276.889006	37.232692
1715.896984	305856.235266	37.237709
1717.235477	306458.276359	37.242727
1719.125317	307047.244754	37.247744
1720.576740	307641.081475	37.252762
1722.344127	308228.919287	37.257780
1724.110585	308830.492532	37.262797
1725.742775	309421.214205	37.267815
1727.563682	310010.173672	37.272832
1729.048641	310620.288098	37.277850
1730.678046	311205.537460	37.282868
1732.096437	311813.292153	37.287885
1733.704821	312414.839896	37.292903
1735.942370	313021.713754	37.297920
1737.320858	313630.806973	37.302938
1739.283674	314240.738582	37.307956
1741.072019	314847.240486	37.312973
1742.650901	315446.941084	37.317991
1744.287355	316065.190227	37.323008
1745.860323	316686.974371	37.328026
1747.966172	317288.325225	37.333044
1749.711543	317892.041314	37.338061
1751.338420	318482.288197	37.343079
1753.297912	319064.501964	37.348096
1755.004893	319652.643607	37.353114
1756.863569	320245.706731	37.358132
1758.382836	320841.131398	37.363149
1759.544990	321436.025744	37.368167
1761.745311	322021.196313	37.373184
1762.655566	322628.334989	37.378202
1764.339051	323233.334619	37.383220
1765.596087	323850.459684	37.388237
1767.744439	324480.152554	37.393255
1769.626685	325097.289477	37.398272
1771.684953	325724.395086	37.403290
1773.452279	326350.882290	37.408308
1774.912528	326981.958591	37.413325
1776.208198	327609.450283	37.418343
1778.412230	328253.771011	37.423360
1780.132371	328907.964794	37.428378
1781.569103	329556.942743	37.433396
1783.244009	330200.212710	37.438413
1784.953559	330856.290869	37.443431
1787.010582	331503.164728	37.448448
1788.593043	332170.318022	37.453466
1789.994955	332842.748447	37.458484
1791.954258	333511.956354	37.463501
1793.500327	334186.784092	37.468519
1795.613495	334865.394176	37.473536
1796.816429	335547.243126	37.478554
1798.799776	336240.175244	37.483572
1801.314142	336918.515896	37.488589
1802.897289	337612.460993	37.493607
1804.769557	338295.002407	37.498624
1806.527246	338983.798396	37.503642
1808.592737	339664.107043	37.508660
1810.465442	340363.577769	37.513677
1812.094462	341052.595862	37.518695
1814.650367	341738.913419	37.523712
1816.191310	342430.110202	37.528730
1817.964117	343108.390390	37.533748
1820.203095	343806.153800	37.538765
1822.160252	344506.441167	37.543783
1824.187221	345191.402126	37.548800
1826.033948	345886.687691	37.553818
1827.929881	346561.092359	37.558836
1829.611674	347249.227999	37.563853
1831.399502	347934.848895	37.568871
1833.431380	348627.119615	37.573888
1834.827459	349319.307230	37.578906
1836.609857	350029.769383	37.583924
1838.709388	350720.804662	37.588941
1840.500520	351424.289986	37.593959
1842.501870	352116.791993	37.598976
1844.191741	352812.887403	37.603994
1846.788049	353492.479853	37.609012
1848.583135	354185.922455	37.614029
1849.938358	354891.378566	37.619047
1851.797727	355574.688861	37.624064
1853.879878	356282.286099	37.629082
1855.530097	356978.575071	37.634100
1857.616005	357676.988275	37.639117
1859.240392	358378.054117	37.644135
1861.120082	359077.898905	37.649152
1862.547637	359778.212419	37.654170
1864.690385	360500.672979	37.659188
1866.756945	361188.627522	37.664205
1868.427414	361905.533854	37.669223
1870.430726	362600.883262	37.674240
1871.861499	363303.799347	37.679258
1873.845290	363983.677163	37.684276
1876.144756	364658.924646	37.689293
1877.692434	365348.947944	37.694311
1879.431739	366030.809386	37.699328
1881.299721	366723.825039	37.704346
1883.264097	367408.060366	37.709364
1885.190862	368087.089307	37.714381
1886.782626	368778.185313	37.719399
1888.955676	369472.521154	37.724416
1890.815643	370158.702526	37.729434
1892.555459	370856.457777	37.734452
1894.785358	371549.806959	37.739469
1896.435658	372254.754202	37.744487
1898.230667	372947.514546	37.749504
1899.845759	373657.310352	37.754522
1901.699305	374371.187050	37.759540
1903.955612	375088.153423	37.764557
1905.366240	375801.136182	37.769575
1907.296574	376520.029556	37.774592
1909.258436	377246.917136	37.779610
1910.939574	377987.353069	37.784628
1913.090487	378720.594926	37.789645
1915.101399	379458.155400	37.794663
1916.884439	380185.695461	37.799680
1918.824809	380928.155480	37.804698
1920.523054	381682.988409	37.809716
1922.389912	382416.121514	37.814733
1923.893145	383179.954750	37.819751
1925.849441	383936.672071	37.824768
1927.431469	384713.616763	37.829786
1929.484958	385479.638766	37.834804
1931.387490	386262.274739	37.839821
1933.329977	387042.121675	37.844839
1935.515439	387812.275491	37.849856
1937.185305	388601.687623	37.854874
1938.819055	389395.015658	37.859892
1941.038386	390178.086736	37.864909
1942.902183	390972.807487	37.869927
1944.918446	391764.567631	37.874944
1946.886754	392561.968369	37.879962
1949.032433	393362.183631	37.884980
1951.021848	394169.678632	37.889997
1952.600718	394986.091483	37.895015
1955.026174	395780.899517	37.900032
1956.790392	396584.539957	37.905050
1958.701014	397390.466431	37.910068
1960.658393	398198.644368	37.915085
1962.567577	399023.636455	37.920103
1964.215317	399835.318044	37.925120
1966.688167	400657.712887	37.930138
1968.555061	401471.618901	37.935156
1970.773748	402288.788961	37.940173
1972.658025	403116.253705	37.945191
1974.763211	403932.356615	37.950208
1976.696754	404758.574526	37.955226
1978.750241	405570.939241	37.960244
1980.899751	406387.698617	37.965261
1982.807741	407224.211065	37.970279
1984.987233	408041.753024	37.975296
1986.729177	408859.342908	37.980314
1988.794969	409684.733960	37.985332
1991.165999	410498.674947	37.990349
1993.052631	411323.159140	37.995367
1994.881426	412144.334513	38.000384
1997.101199	412964.559002	38.005402
1998.736703	413804.916290	38.010420
2000.669103	414623.465213	38.015437
2002.386887	415443.797152	38.020455
2004.391293	416241.590224	38.025472
2006.609363	417056.672836	38.030490
2008.182310	417859.046402	38.035508
2010.499337	418654.864936	38.040525
2012.355872	419471.982338	38.045543
2014.363596	420278.893743	38.050560
2016.231839	421084.181862	38.055578
2017.810234	421906.610128	38.060596
2019.996793	422728.151580	38.065613
2022.126167	423558.715025	38.070631
2024.355327	424393.108269	38.075648
2026.420112	425201.168696	38.080666
2028.224157	426043.779721	38.085684
2030.411541	426866.297875	38.090701
2032.323975	427715.821045	38.095719
2033.857365	428550.744591	38.100736
2036.005049	429400.625559	38.105754
2037.625791	430263.017779	38.110772
2039.802776	431124.173400	38.115789
2041.566569	431993.212705	38.120807
2043.641828	432858.473325	38.125824
2046.083925	433729.361736	38.130842
2047.839111	434605.291647	38.135860
2050.043109	435480.001064	38.140877
2051.860173	436362.181625	38.145895
2054.083604	437252.308830	38.150912
2056.264721	438138.764530	38.155930
2058.366779	439036.433959	38.160948
2060.236857	439918.620560	38.165965
2062.627814	440831.808652	38.170983
2064.175038	441732.448176	38.176000
2066.828037	442624.165807	38.181018
2068.787641	443535.138874	38.186036
2071.042125	444426.040282	38.191053
2073.126121	445344.457089	38.196071
2075.387180	446246.768514	38.201088
2077.456060	447142.244652	38.206106
2079.515128	448055.391271	38.211124
2082.085898	448956.122548	38.216141
2084.522848	449863.869286	38.221159
2086.333705	450767.128413	38.226176
2088.424603	451667.268271	38.231194
2090.351499	452582.721842	38.236212
2092.635546	453486.899680	38.241229
2094.451450	454404.365847	38.246247
2096.778969	455319.633940	38.251264
2098.875956	456224.330937	38.256282
2100.757376	457144.244333	38.261300
2103.332843	458055.355735	38.266317
2105.039533	458989.979921	38.271335
2106.923588	459908.403598	38.276352
2109.254812	460823.122416	38.281370
2110.870325	461763.043528	38.286388
2113.129246	462685.222376	38.291405
2115.416311	463628.736725	38.296423
2117.504833	464555.507849	38.301440
2119.830198	465488.716913	38.306458
2121.647963	466420.853591	38.311476
2124.404798	467346.979009	38.316493
2126.499738	468276.555733	38.321511
2128.594661	469217.205877	38.326528
2130.610491	470138.923970	38.331546
2132.748162	471086.196982	38.336564
2134.975103	472015.774160	38.341581
2137.032472	472954.327649	38.346599
2138.959251	473895.230941	38.351616
2141.223645	474824.007854	38.356634
2143.060344	475776.401537	38.361652
2145.255853	476679.636951	38.366669
2146.844237	477589.242966	38.371687
2148.795022	478513.190833	38.376704
2151.315558	479434.271200	38.381722
2153.121407	480366.181120	38.386740
2155.127936	481285.687868	38.391757
2157.389013	482218.438550	38.396775
2159.511090	483165.051291	38.401792
2161.740600	484099.528475	38.406810
2163.590416	485056.741585	38.411828
2165.400299	486002.247085	38.416845
2168.075155	486954.527223	38.421863
2170.237724	487910.980639	38.426880
2172.730866	488866.823129	38.431898
2174.797262	489821.523208	38.436916
2176.967101	490784.533457	38.441933
2179.153583	491745.670925	38.446951
2180.986522	492708.125922	38.451968
2183.127406	493681.478782	38.456986
2185.196567	494666.395609	38.462004
2186.810919	495654.863398	38.467021
2189.167402	496643.202236	38.472039
2190.910376	497646.267746	38.477056
2193.137870	498657.165733	38.482074
2195.018723	499667.606377	38.487092
2197.755047	500684.050312	38.492109
2200.337389	501698.541097	38.497127
2202.627335	502720.685447	38.502144
2205.257890	503729.395115	38.507162
2207.495182	504751.826394	38.512180
2209.432785	505767.939648	38.517197
2212.145985	506776.096046	38.522215
2214.044350	507805.049423	38.527232
2216.603878	508827.727573	38.532250
2218.354144	509859.398728	38.537268
2220.485377	510884.034078	38.542285
2223.175195	511905.285509	38.547303
2225.283092	512952.478044	38.552320
2227.333335	513990.941350	38.557338
2229.591777	515028.899058	38.562356
2232.003871	516064.343986	38.567373
2234.331867	517112.535146	38.572391
2236.143639	518158.775892	38.577408
2238.231971	519201.625491	38.582426
2240.314941	520265.517558	38.587444
2242.542254	521325.080452	38.592461
2244.821016	522382.294839	38.597479
2247.291319	523455.071430	38.602496
2249.324089	524521.447498	38.607514
2251.288315	525593.149422	38.612532
2253.361081	526664.556069	38.617549
2255.981396	527751.106003	38.622567
2258.161056	528831.506275	38.627584
2260.515841	529910.792451	38.632602
2262.724468	530997.425878	38.637620
2264.981314	532080.548083	38.642637
2267.366810	533171.271976	38.647655
2269.880446	534250.970194	38.652672
2272.401377	535344.530370	38.657690
2274.202418	536428.815832	38.662708
2276.238926	537519.826007	38.667725
2278.640121	538602.742503	38.672743
2281.197809	539702.308272	38.677760
2283.685405	540799.436362	38.682778
2286.143721	541898.296174	38.687796
2288.337466	542985.040630	38.692813
2290.668447	544076.357355	38.697831
2292.691808	545160.900038	38.702848
2295.102077	546228.496039	38.707866
2297.151138	547284.905058	38.712884
2299.671793	548343.318667	38.717901
2302.438196	549392.408815	38.722919
2304.269581	550458.769803	38.727936
2306.414596	551518.762106	38.732954
2308.656640	552589.415102	38.737972
2310.509435	553658.942475	38.742989
2312.596352	554734.328873	38.748007
2315.034911	555812.788791	38.753024
2317.279362	556905.467825	38.758042
2319.654561	557982.658974	38.763060
2321.727259	559077.752562	38.768077
2324.413595	560182.603788	38.773095
2326.280510	561289.256794	38.778112
2328.891158	562397.603788	38.783130
2331.566921	563502.380920	38.788148
2333.919849	564611.990629	38.793165
2336.388561	565712.949126	38.798183
2338.397862	566844.374039	38.803200
2341.126964	567955.746638	38.808218
2343.475631	569090.083346	38.813236
2345.046833	570216.214562	38.818253
2347.530374	571343.150943	38.823271
2349.821455	572491.303788	38.828288
2351.960329	573642.239371	38.833306
2354.367013	574794.080481	38.838324
2356.392831	575957.170979	38.843341
2359.212478	577108.130701	38.848359
2361.234153	578278.935576	38.853376
2363.999610	579447.752261	38.858394
2366.415544	580620.780961	38.863412
2368.498332	581795.358837	38.868429
2371.245915	582968.862851	38.873447
2373.908063	584150.493890	38.878464
2376.292028	585321.776938	38.883482
2379.155454	586484.043735	38.888500
2381.437043	587646.445866	38.893517
2383.814511	588821.504412	38.898535
2386.161707	590000.413680	38.903552
2388.932951	591166.556885	38.908570
2391.675848	592345.471452	38.913588
2393.669135	593522.338614	38.918605
2395.953907	594691.875977	38.923623
2398.497744	595891.567157	38.928640
2400.987943	597055.225562	38.933658
2403.468520	598244.718270	38.938676
2405.813932	599435.064197	38.943693
2408.556136	600611.601041	38.948711
2410.895647	601797.449676	38.953728
2413.450625	602976.081329	38.958746
2415.865673	604157.269286	38.963764
2418.129303	605347.722457	38.968781
2420.437668	606522.126688	38.973799
2422.777387	607717.927023	38.978816
2425.158807	608913.294547	38.983834
2427.485942	610100.138154	38.988852
2429.692044	611304.439432	38.993869
2432.375349	612492.223396	38.998887
2434.971606	613703.157365	39.003904
2438.070375	614887.617125	39.008922
2441.341712	616066.470860	39.013940
2443.775318	617235.685704	39.018957
2446.213428	618407.226293	39.023975
2448.650428	619588.142088	39.028992
2451.015534	620754.644759	39.034010
2453.325312	621935.728422	39.039028
2455.449268	623103.469516	39.044045
2457.928062	624252.635170	39.049063
2459.916534	625410.354712	39.054080
2462.116043	626564.417606	39.059098
2464.606164	627722.405472	39.064116
2466.223573	628883.659121	39.069133
2468.772194	630050.676899	39.074151
2470.835311	631224.888618	39.079168
2473.159569	632404.120893	39.084186
2475.858454	633591.248972	39.089204
2477.494828	634788.853186	39.094221
2479.883436	635991.338686	39.099239
2482.278205	637217.943974	39.104256
2484.340334	638442.662977	39.109274
2486.729078	639666.235546	39.114292
2488.754330	640930.440081	39.119309
2491.323644	642173.345633	39.124327
2493.535279	643437.211566	39.129344
2496.097310	644712.385887	39.134362
2498.368806	645988.595781	39.139380
2500.914551	647274.523754	39.144397
2504.108527	648552.852091	39.149415
2506.377428	649834.710610	39.154432
2509.167754	651133.567115	39.159450
2511.944255	652422.687965	39.164468
2514.129143	653733.567521	39.169485
2516.742773	655024.471657	39.174503
2519.500721	656338.749548	39.179520
2522.121770	657642.912060	39.184538
2524.713024	658951.638426	39.189556
2527.355937	660265.809178	39.194573
2530.351746	661567.395775	39.199591
2533.295724	662870.161143	39.204608
2536.099060	664173.172951	39.209626
2538.863749	665470.988170	39.214644
2541.256024	666784.217597	39.219661
2543.553267	668087.380460	39.224679
2546.069763	669408.191539	39.229696
2548.492406	670719.581937	39.234714
2551.413776	672042.895535	39.239732
2553.266884	673361.077545	39.244749
2555.898117	674681.184749	39.249767
2558.424836	676024.392590	39.254784
2560.803056	677351.325290	39.259802
2563.253725	678690.632845	39.264820
2565.748533	680044.848483	39.269837
2568.253305	681387.137412	39.274855
2570.865073	682745.559496	39.279872
2573.511253	684100.248253	39.284890
2575.967244	685448.311134	39.289908
2578.742344	686797.860605	39.294925
2581.090759	688153.139495	39.299943
2584.185487	689513.405068	39.304960
2586.584647	690886.337845	39.309978
2589.704385	692238.444581	39.314996
2592.201835	693608.563028	39.320013
2594.193582	694962.032523	39.325031
2597.014575	696335.003467	39.330048
2599.146041	697713.976746	39.335066
2602.066335	699083.430291	39.340084
2604.591474	700453.876744	39.345101
2607.256741	701836.679240	39.350119
2610.404958	703210.558512	39.355136
2612.609096	704592.059249	39.360154
2615.440218	705963.375796	39.365172
2618.130427	707350.303987	39.370189
2620.554634	708725.708872	39.375207
2623.660556	710101.475015	39.380224
2625.524796	711467.617632	39.385242
2628.291569	712818.390072	39.390260
2630.834079	714162.648329	39.395277
2633.464012	715509.797805	39.400295
2636.056258	716856.244102	39.405312
2638.397131	718199.597325	39.410330
2641.099809	719556.826313	39.415348
2644.356825	720898.507984	39.420365
2647.059499	722236.009700	39.425383
2649.686855	723588.787316	39.430400
2652.275253	724954.947762	39.435418
2654.571523	726303.974232	39.440436
2657.232105	727669.624012	39.445453
2659.737297	729042.584043	39.450471
2662.410635	730408.566228	39.455488
2664.574582	731798.314485	39.460506
2667.365333	733179.621341	39.465524
2669.822410	734583.020639	39.470541
2672.273091	735983.708341	39.475559
2675.292812	737385.835830	39.480576
2677.736683	738805.631995	39.485594
2680.683200	740214.581537	39.490612
2683.146272	741651.387907	39.495629
2685.379394	743071.495058	39.500647
2688.397509	744494.769442	39.505664
2690.780927	745938.160202	39.510682
2693.660030	747381.155014	39.515700
2696.148096	748839.131997	39.520717
2698.713428	750309.934572	39.525735
2701.354230	751767.732955	39.530752
2704.297123	753240.579486	39.535770
2706.664675	754716.195751	39.540788
2709.617290	756185.079673	39.545805
2711.941982	757681.360753	39.550823
2715.208514	759162.621629	39.555840
2717.925758	760654.513906	39.560858
2720.775568	762134.871128	39.565876
2723.475280	763627.903801	39.570893
2726.108424	765131.671098	39.575911
2729.010802	766632.191570	39.580928
2731.590827	768149.625901	39.585946
2734.189270	769648.018007	39.590964
2736.883348	771165.852022	39.595981
2739.816893	772693.115305	39.600999
2742.579829	774205.842792	39.606016
2745.010658	775729.759815	39.611034
2747.840810	777257.714768	39.616052
2750.442813	778786.713934	39.621069
2753.239107	780328.369597	39.626087
2756.157366	781856.426230	39.631104
2758.468161	783397.951123	39.636122
2761.774183	784938.982711	39.641140
2764.074013	786491.474518	39.646157
2766.656423	788044.613264	39.651175
2769.983006	789603.567175	39.656192
2772.226127	791161.426782	39.661210
2775.097285	792717.321538	39.666228
2777.722953	794296.089097	39.671245
2780.115866	795870.132551	39.676263
2783.198745	797434.649255	39.681280
2785.825846	799018.867803	39.686298
2788.673306	800586.878738	39.691316
2791.702592	802169.970893	39.696333
2794.334909	803764.313662	39.701351
2797.193477	805339.221742	39.706368
2799.871194	806929.937977	39.711386
2802.695978	808517.620341	39.716404
2805.252311	810108.986223	39.721421
2808.069264	811695.440766	39.726439
2810.829926	813248.112610	39.731456
2813.412911	814809.152280	39.736474
2816.453290	816361.891842	39.741492
2819.116586	817915.945690	39.746509
2821.717657	819476.043719	39.751527
2824.884567	821032.462469	39.756544
2827.345131	822602.831830	39.761562
2830.265914	824167.338406	39.766580
2833.000267	825750.525093	39.771597
2835.719853	827328.750088	39.776615
2838.552330	828925.246392	39.781632
2841.068403	830507.028358	39.786650
2843.685206	832097.569441	39.791668
2846.829188	833716.178128	39.796685
2849.679545	835313.977190	39.801703
2852.505897	836919.514858	39.806720
2854.917951	838548.813116	39.811738
2857.978975	840166.106021	39.816756
2860.728596	841805.564825	39.821773
2863.374381	843443.596907	39.826791
2866.609888	845083.928798	39.831808
2869.117154	846742.329687	39.836826
2872.120253	848387.090706	39.841844
2875.164762	850049.001628	39.846861
2877.798159	851722.778817	39.851879
2881.094090	853383.177765	39.856896
2883.506234	855057.745153	39.861914
2886.895721	856734.901665	39.866932
2889.893174	858406.038456	39.871949
2892.724087	860093.725605	39.876967
2895.901221	861758.196054	39.881984
2899.227368	863450.985098	39.887002
2902.077897	865136.305447	39.892020
2905.042621	866802.435789	39.897037
2908.078366	868497.739902	39.902055
2911.193563	870188.001658	39.907072
2914.091778	871869.980363	39.912090
2917.139478	873564.625774	39.917108
2920.120744	875247.284802	39.922125
2923.022156	876926.094394	39.927143
2925.781419	878627.179164	39.932160
2928.831884	880318.637028	39.937178
2931.809296	882009.427035	39.942196
2935.109562	883717.262706	39.947213
2937.910693	885401.883096	39.952231
2941.151112	887090.482517	39.957248
2943.688207	888795.408677	39.962266
2947.090994	890487.914331	39.967284
2950.015631	892183.378662	39.972301
2952.597138	893892.385672	39.977319
2955.801294	895603.769138	39.982336
2958.542479	897305.460720	39.987354
2961.529648	898995.423017	39.992372
2964.362351	900712.461236	39.997389
2966.891025	902431.531593	40.002407
2970.454013	904145.766113	40.007424
2973.094973	905879.938533	40.012442
2976.088357	907595.905456	40.017460
2979.131361	909317.780749	40.022477
2982.452842	911038.595251	40.027495
2985.278737	912759.340710	40.032512
2987.942693	914498.604979	40.037530
2990.840070	916222.484665	40.042548
2994.307747	917938.908554	40.047565
2996.761862	919688.853135	40.052583
2999.796308	921424.605474	40.057600
3002.472459	923155.735158	40.062618
3005.505626	924881.647171	40.067636
3008.519780	926581.214139	40.072653
3010.862420	928292.144695	40.077671
3013.695133	930007.334850	40.082688
3016.653718	931712.755751	40.087706
3018.968341	933430.664465	40.092724
3021.706949	935160.966738	40.097741
3024.258796	936905.375913	40.102759
3027.147574	938650.682176	40.107776
3030.063089	940422.278872	40.112794
3032.679388	942183.859035	40.117812
3035.367343	943983.349488	40.122829
3037.877859	945783.774195	40.127847
3041.022404	947574.776507	40.132864
3043.899452	949402.341426	40.137882
3046.488109	951233.694242	40.142900
3049.504327	953076.724796	40.147917
3052.049614	954945.718169	40.152935
3055.080463	956860.528477	40.157952
3058.172282	958782.321944	40.162970
3061.162532	960722.164824	40.167988
3063.846575	962670.298856	40.173005
3066.745039	964624.870559	40.178023
3070.303174	966583.455245	40.183040
3073.432387	968552.768444	40.188058
3076.169342	970539.038488	40.193076
3079.584874	972511.143264	40.198093
3081.891202	974506.549534	40.203111
3085.397772	976519.977081	40.208128
3088.229750	978526.472507	40.213146
3090.943436	980547.676672	40.218164
3094.402677	982579.924686	40.223181
3097.650350	984619.856550	40.228199
3100.478486	986651.925939	40.233216
3103.350155	988695.618764	40.238234
3106.492338	990750.689655	40.243252
3110.350178	992800.427934	40.248269
3112.901742	994872.965211	40.253287
3115.787665	996934.684607	40.258304
3118.380600	999017.358160	40.263322
3121.925230	1001098.720936	40.268340
3125.315338	1003181.672508	40.273357
3128.206048	1005271.214080	40.278375
3131.203885	1007384.109647	40.283392
3134.479671	1009473.777350	40.288410
3137.201013	1011592.508240	40.293428
3140.692832	1013700.532491	40.298445
3143.796935	1015811.219432	40.303463
3146.838083	1017928.576524	40.308480
3150.240107	1020046.526934	40.313498
3153.348038	1022170.109027	40.318516
3156.840254	1024294.659879	40.323533
3160.150125	1026413.409233	40.328551
3163.437096	1028527.302361	40.333568
3166.908001	1030652.435999	40.338586
3169.797373	1032771.643713	40.343604
3173.603305	1034884.394989	40.348621
3176.742242	1036997.612176	40.353639
3179.503613	1039115.199245	40.358656
3182.534679	1041237.814594	40.363674
3186.032331	1043364.455410	40.368692
3189.347750	1045481.161791	40.373709
3192.173164	1047592.808292	40.378727
3195.762688	1049716.226580	40.383744
3198.437596	1051838.018365	40.388762
3201.438870	1053969.230894	40.393780
3205.106847	1056099.991446	40.398797
3207.779318	1058234.032175	40.403815
3210.902491	1060352.956859	40.408832
3214.290014	1062447.019166	40.413850
3217.143597	1064537.972437	40.418868
3220.069574	1066615.453826	40.423885
3223.171970	1068713.697809	40.428903
3226.430801	1070816.097918	40.433920
3229.565623	1072910.140793	40.438938
3232.017769	1075026.005815	40.443956
3235.342107	1077136.120346	40.448973
3238.569853	1079260.175831	40.453991
3241.584295	1081384.109036	40.459008
3244.566751	1083531.895551	40.464026
3247.825590	1085687.489149	40.469044
3251.074356	1087838.311604	40.474061
3254.071982	1090013.734538	40.479079
3257.142765	1092178.151296	40.484096
3260.491944	1094356.166766	40.489114
3263.285767	1096551.526292	40.494132
3266.569605	1098740.573169	40.499149
3269.881266	1100948.558593	40.504167
3273.373690	1103160.757098	40.509184
3277.019378	1105370.308090	40.514202
3280.047764	1107594.860625	40.519220
3283.337788	1109818.069656	40.524237
3286.789494	1112043.472062	40.529255
3290.215512	1114280.604594	40.534272
3293.515491	1116513.687701	40.539290
3296.702778	1118768.758546	40.544308
3300.066122	1121003.284145	40.549325
3303.572047	1123270.935942	40.554343
3306.308977	1125532.626772	40.559360
3309.542098	1127784.739553	40.564378
3312.736341	1130064.637206	40.569396
3316.011743	1132334.825197	40.574413
3319.343691	1134616.634675	40.579431
3322.501083	1136906.583409	40.584448
3326.180453	1139206.343117	40.589466
3329.126839	1141515.159925	40.594484
3332.736445	1143805.931608	40.599501
3335.995401	1146121.953999	40.604519
3339.305550	1148427.408566	40.609536
3342.721848	1150735.521530	40.614554
3345.796870	1153052.025995	40.619572
3349.086845	1155381.064244	40.624589
3352.607250	1157705.731261	40.629607
3355.723501	1160036.223978	40.634624
3359.688361	1162366.295309	40.639642
3362.847323	1164714.585292	40.644660
3366.361388	1167044.061467	40.649677
3369.519541	1169379.898931	40.654695
3373.092236	1171719.702917	40.659712
3376.622529	1174062.319179	40.664730
3379.781210	1176407.984435	40.669748
3383.119514	1178749.368342	40.674765
3386.572687	1181099.819860	40.679783
3389.840803	1183468.666498	40.684800
3393.817764	1185817.644287	40.689818
3397.148360	1188187.418599	40.694836
3400.382308	1190540.094847	40.699853
3404.149982	1192900.886950	40.704871
3407.330274	1195256.294186	40.709888
3410.789661	1197616.569589	40.714906
3414.383441	1199968.442869	40.719924
3417.661422	1202323.781150	40.724941
3420.792199	1204694.234535	40.729959
3424.119488	1207060.009713	40.734976
3427.807475	1209428.088392	40.739994
3431.088825	1211801.858927	40.745012
3434.447350	1214154.040641	40.750016
3437.987460	1216454.783172	40.755021
3440.831109	1218705.537517	40.760026
3444.361771	1220878.022136	40.765031
3446.980165	1222999.398632	40.770036
3450.184464	1225037.747342	40.775040
3453.328571	1227002.603766	40.780045
3456.540973	1228893.564695	40.785050
3459.099596	1230682.766570	40.790055
3461.953554	1232426.922156	40.795060
3465.086743	1234070.641457	40.800064
3467.996961	1235631.336414	40.805069
3470.231785	1237118.656028	40.810074
3472.643496	1238529.080019	40.815079
3475.064627	1239875.915600	40.820084
3477.234125	1241130.412832	40.825088
3479.464303	1242316.588767	40.830093
3481.764718	1243441.557984	40.835098
3484.123567	1244498.668599	40.840103
3485.843315	1245491.703683	40.845108
3487.613344	1246408.597549	40.850112
3489.917679	1247279.886201	40.855117
3491.142863	1248094.244580	40.860122
3492.622068	1248830.949670	40.865127
3494.129720	1249531.779867	40.870132
3495.712435	1250177.795713	40.875136
3496.966071	1250772.799536	40.880141
3498.004086	1251332.669063	40.885146
3499.757437	1251837.022414	40.890151
3500.692242	1252318.064890	40.895156
3501.606117	1252734.641584	40.900160
3502.732229	1253126.736552	40.905165
3503.688464	1253465.738542	40.910170
3504.986383	1253786.006581	40.915175
3505.561084	1254074.912656	40.920180
3506.594187	1254321.688477	40.925184
3507.596392	1254543.309667	40.930189
3508.090918	1254726.310453	40.935194
3508.811928	1254875.028075	40.940199
3509.483677	1255012.336611	40.945204
3510.065789	1255122.191910	40.950208
3511.024888	1255210.549847	40.955213
3511.307330	1255283.987023	40.960218
3511.687158	1255322.428742	40.965223
3511.831728	1255348.569103	40.970228
3512.986314	1255341.977077	40.975232
3513.740881	1255328.306790	40.980237
3514.186666	1255296.594950	40.985242
3514.536335	1255244.950540	40.990247
3515.145526	1255176.376242	40.995252
3515.379132	1255076.779773	41.000256
3516.058042	1254986.665088	41.005261
3515.840403	1254861.065341	41.010266
3516.465519	1254729.756132	41.015271
3516.763124	1254605.178613	41.020276
3516.806144	1254441.293973	41.025280
3517.364285	1254284.835964	41.030285
3517.753763	1254124.781515	41.035290
3518.174315	1253920.262444	41.040295
3518.263298	1253738.435418	41.045300
3518.616630	1253534.004444	41.050304
3518.661781	1253307.339499	41.055309
3518.684552	1253090.043051	41.060314
3519.232174	1252849.072750	41.065319
3519.504277	1252621.782426	41.070324
3520.111285	1252368.711172	41.075328
3520.050115	1252101.903913	41.080333
3520.064423	1251841.476358	41.085338
3520.522733	1251573.534099	41.090343
3520.427574	1251296.383097	41.095348
3520.330529	1251015.874077	41.100352
3520.769332	1250725.788752	41.105357
3520.524751	1250428.648057	41.110362
3520.955568	1250127.756297	41.115367
3520.778078	1249835.306117	41.120372
3521.292824	1249522.753869	41.125376
3521.332145	1249202.178622	41.130381
3521.176651	1248900.287922	41.135386
3521.635760	1248576.816569	41.140391
3521.246217	1248256.530220	41.145396
3521.580215	1247934.803410	41.150400
3521.788882	1247609.266735	41.155405
3521.253721	1247266.174702	41.160410
3521.749203	1246932.090205	41.165415
3521.728188	1246594.629661	41.170420
3521.966898	1246251.712617	41.175424
3522.071910	1245919.298140	41.180429
3522.100527	1245574.696281	41.185434
3522.512750	1245216.248322	41.190439
3521.968836	1244862.209104	41.195444
3522.024553	1244506.651462	41.200448
3522.209328	1244153.837057	41.205453
3521.949191	1243797.165395	41.210458
3522.284918	1243429.954158	41.215463
3522.290629	1243084.069284	41.220468
3522.237148	1242720.218612	41.225472
3522.361315	1242348.312539	41.230477
3522.109151	1241987.418276	41.235482
3522.281587	1241608.472476	41.240487
3522.298604	1241240.223571	41.245492
3522.624978	1240871.803738	41.250496
3522.517916	1240496.542230	41.255501
3522.198915	1240133.851085	41.260506
3522.363345	1239760.165127	41.265511
3522.611294	1239379.363918	41.270516
3522.184780	1239012.048981	41.275520
3522.618514	1238623.620357	41.280525
3522.378658	1238240.486194	41.285530
3522.585415	1237865.163224	41.290535
3522.464484	1237484.745180	41.295540
3522.333918	1237105.510568	41.300544
3522.510369	1236728.990642	41.305549
3522.454265	1236339.349286	41.310554
3522.412503	1235952.190254	41.315559
3522.189114	1235571.924284	41.320564
3522.466155	1235192.851407	41.325568
3522.536546	1234807.542362	41.330573
3522.274663	1234419.836287	41.335578
3522.420207	1234028.306361	41.340583
3522.102552	1233654.433781	41.345588
3522.234864	1233260.703387	41.350592
3522.452723	1232882.957990	41.355597
3522.271540	1232500.589940	41.360602
3522.270986	1232100.732901	41.365607
3522.340603	1231728.052232	41.370612
3522.346023	1231333.540174	41.375616
3522.576358	1230943.435448	41.380621
3522.209099	1230537.082226	41.385626
3522.548136	1230145.872506	41.390631
3522.264454	1229748.673627	41.395636
3521.890203	1229366.007215	41.400640
3522.147016	1228975.373451	41.405645
3522.201949	1228583.063866	41.410650
3522.413343	1228183.048976	41.415655
3522.295769	1227797.889779	41.420660
3522.150339	1227400.950494	41.425664
3522.404143	1227015.204192	41.430669
3522.047870	1226610.213570	41.435674
3522.256563	1226212.003165	41.440679
3522.225236	1225832.932872	41.445684
3521.899791	1225431.296104	41.450688
3522.125049	1225031.216985	41.455693
3521.928505	1224650.218749	41.460698
3522.093855	1224246.353749	41.465703
3522.030376	1223854.164612	41.470708
3521.939642	1223459.428705	41.475712
3521.760143	1223071.586617	41.480717
3521.769042	1222680.322083	41.485722
3522.008269	1222285.907593	41.490727
3521.448302	1221893.462087	41.495732
3521.564625	1221497.792522	41.500736
3521.799382	1221114.403145	41.505741
3521.447327	1220724.635558	41.510746
3521.548314	1220324.393099	41.515751
3521.743211	1219950.358698	41.520756
3521.718922	1219563.905269	41.525760
3521.569859	1219175.106847	41.530765
3521.456479	1218774.123652	41.535770
3521.050095	1218379.325680	41.540775
3520.740237	1218003.175169	41.545780
3520.882830	1217616.452980	41.550784
3521.732707	1217233.511288	41.555789
3521.402450	1216863.730397	41.560794
3521.723207	1216460.623796	41.565799
3521.292419	1216067.146636	41.570804
3521.255958	1215679.184906	41.575808
3521.387192	1215293.971630	41.580813
3521.505921	1214902.184476	41.585818
3521.336648	1214507.047458	41.590823
3521.361876	1214118.863383	41.595828
3521.396999	1213725.503016	41.600832
3521.328422	1213331.568090	41.605837
3521.195200	1212940.700981	41.610842
3521.144403	1212547.638281	41.615847
3521.201530	1212170.342030	41.620852
3521.153055	1211778.342683	41.625856
3521.215911	1211383.206431	41.630861
3520.808710	1210997.851253	41.635866
3520.732249	1210609.978818	41.640871
3520.796104	1210233.942595	41.645876
3520.882293	1209847.296100	41.650880
3521.013640	1209456.025262	41.655885
3520.732432	1209077.058412	41.660890
3520.804182	1208688.079501	41.665895
3520.945805	1208292.691496	41.670900
3520.772679	1207900.790019	41.675904
3520.874561	1207516.868169	41.680909
3520.556094	1207136.452509	41.685914
3520.716742	1206738.412314	41.690919
3520.462529	1206367.952319	41.695924
3520.476551	1205973.530482	41.700928
3520.748882	1205589.810917	41.705933
3520.332441	1205209.643113	41.710938
3520.642962	1204831.201610	41.715943
3520.358411	1204451.424421	41.720948
3520.584885	1204066.192639	41.725952
3520.319004	1203687.574244	41.730957
3520.445073	1203300.051920	41.735962
3520.707801	1202909.290474	41.740967
3520.496693	1202536.671632	41.745972
3520.180936	1202146.603673	41.750976
3520.220943	1201762.542340	41.755981
3519.863933	1201395.396943	41.760986
3520.217687	1201010.665089	41.765991
3520.445003	1200642.150489	41.770996
3520.092657	1200255.508856	41.776000
3520.281048	1199872.688740	41.781005
3519.815029	1199500.266802	41.786010
3519.844037	1199114.226988	41.791015
3520.040579	1198739.013976	41.796020
3519.904617	1198363.453044	41.801024
3519.996532	1197985.481275	41.806029
3519.568580	1197613.948658	41.811034
3519.837585	1197231.669450	41.816039
3519.875226	1196866.575673	41.821044
3519.679885	1196489.386059	41.826048
3519.585111	1196108.021976	41.831053
3519.199937	1195751.179303	41.836058
3519.373318	1195376.382120	41.841063
3519.419064	1195012.751616	41.846068
3519.060179	1194650.758334	41.851072
3519.506037	1194276.305769	41.856077
3519.482450	1193924.159994	41.861082
3519.366989	1193540.449366	41.866087
3519.400396	1193164.763107	41.871092
3519.452568	1192811.026077	41.876096
3519.540940	1192438.753313	41.881101
3519.276002	1192072.806098	41.886106
3519.427345	1191708.173628	41.891111
3519.231984	1191330.700413	41.896116
3519.195962	1190956.180199	41.901120
3519.400626	1190593.527441	41.906125
3518.889800	1190225.892296	41.911130
3518.870089	1189851.195294	41.916135
3518.964491	1189496.942264	41.921140
3519.060815	1189136.178855	41.926144
3519.108813	1188768.159955	41.931149
3519.055775	1188406.994246	41.936154
3519.191292	1188039.191082	41.941159
3519.103512	1187680.612836	41.946164
3518.903879	1187318.455016	41.951168
3519.039619	1186946.060654	41.956173
3518.592465	1186584.362393	41.961178
3518.756450	1186223.478697	41.966183
3518.446940	1185862.271598	41.971188
3518.723984	1185501.507073	41.976192
3519.146452	1185135.331507	41.981197
3518.426996	1184789.074098	41.986202
3518.683110	1184421.746578	41.991207
3518.648752	1184060.744834	41.996212
3518.432852	1183704.923097	42.001216
3518.542877	1183340.742267	42.006221
3518.396798	1182975.636945	42.011226
3518.062523	1182627.101194	42.016231
3518.568927	1182269.179651	42.021236
3517.988633	1181923.743156	42.026240
3518.298315	1181561.287034	42.031245
3518.234413	1181220.519522	42.036250
3518.195794	1180865.980010	42.041255
3518.332247	1180505.267466	42.046260
3518.111266	1180156.170415	42.051264
3518.162526	1179794.669253	42.056269
3518.068757	1179458.593481	42.061274
3517.816316	1179106.134972	42.066279
3518.106352	1178749.889973	42.071284
3517.890293	1178389.088498	42.076288
3517.989205	1178038.477727	42.081293
3517.446730	1177695.296898	42.086298
3517.319039	1177357.300895	42.091303
3517.455910	1177018.202963	42.096308
3517.178392	1176675.288023	42.101312
3517.489681	1176339.509149	42.106317
3517.253899	1175996.165645	42.111322
3517.510727	1175663.084916	42.116327
3517.512003	1175313.531635	42.121332
3517.330787	1174967.660838	42.126336
3517.368172	1174631.439853	42.131341
3517.087778	1174303.356373	42.136346
3517.142895	1173962.187419	42.141351
3517.134229	1173627.700380	42.146356
3516.993077	1173296.042210	42.151360
3517.105533	1172947.160307	42.156365
3516.541916	1172625.240924	42.161370
3516.860312	1172295.046395	42.166375
3517.036745	1171963.722635	42.171380
3516.601025	1171626.631144	42.176384
3516.852983	1171292.422857	42.181389
3516.804591	1170976.258957	42.186394
3516.647176	1170659.433524	42.191399
3516.767619	1170319.713323	42.196404
3516.492889	1169983.715508	42.201408
3516.761081	1169654.022454	42.206413
3516.410376	1169327.807321	42.211418
3516.493341	1169007.256449	42.216423
3516.477082	1168687.551548	42.221428
3516.264616	1168359.932018	42.226432
3516.260632	1168025.556656	42.231437
3516.196164	1167706.932217	42.236442
3516.095992	1167383.197107	42.241447
3516.194188	1167061.486003	42.246452
3516.185987	1166738.734188	42.251456
3516.332105	1166432.080877	42.256461
3516.167203	1166109.599251	42.261466
3516.141888	1165787.263583	42.266471
3515.871069	1165472.502535	42.271476
3516.095383	1165163.495736	42.276480
3516.456149	1164843.682410	42.281485
3516.235988	1164528.384022	42.286490
3515.777187	1164200.449834	42.291495
3515.726611	1163884.990295	42.296500
3515.799792	1163574.686659	42.301504
3515.846055	1163251.521742	42.306509
3516.094759	1162947.103347	42.311514
3515.963560	1162620.338798	42.316519
3516.131961	1162303.803158	42.321524
3516.227257	1161997.937627	42.326528
3515.977129	1161662.628964	42.331533
3515.741291	1161345.251537	42.336538
3515.768483	1161027.433546	42.341543
3516.005885	1160719.201836	42.346548
3515.872616	1160405.720103	42.351552
3515.743257	1160082.388611	42.356557
3515.211661	1159784.626112	42.361562
3515.324105	1159467.172141	42.366567
3515.579518	1159159.129375	42.371572
3515.307311	1158851.722691	42.376576
3515.443948	1158541.772346	42.381581
3515.379714	1158243.088956	42.386586
3515.217867	1157920.575121	42.391591
3515.118822	1157623.280623	42.396596
3515.220316	1157328.962584	42.401600
3515.289898	1157010.705075	42.406605
3515.063863	1156710.542469	42.411610
3515.004132	1156412.889221	42.416615
3514.991908	1156108.022110	42.421620
3514.775457	1155813.293129	42.426624
3514.932721	1155515.269496	42.431629
3514.828853	1155215.474373	42.436634
3514.656243	1154919.741955	42.441639
3514.740797	1154623.288199	42.446644
3514.755968	1154322.381710	42.451648
3515.024195	1154036.462798	42.456653
3515.076586	1153731.825758	42.461658
3514.716478	1153435.283635	42.466663
3514.562135	1153139.353440	42.471668
3514.167104	1152850.261264	42.476672
3514.588942	1152554.676565	42.481677
3514.476271	1152273.457502	42.486682
3514.655962	1151965.005336	42.491687
3514.464285	1151680.832890	42.496692
3514.252426	1151395.512278	42.501696
3514.388230	1151101.218612	42.506701
3514.567687	1150810.783598	42.511706
3514.383525	1150525.695375	42.516711
3514.179469	1150245.235298	42.521716
3514.347622	1149952.955565	42.526720
3514.210009	1149660.141721	42.531725
3514.030588	1149377.358347	42.536730
3514.147438	1149089.869698	42.541735
3514.182325	1148815.356298	42.546740
3514.020385	1148526.367233	42.551744
3514.174730	1148239.962848	42.556749
3514.014948	1147963.731935	42.561754
3513.977454	1147668.706704	42.566759
3514.389391	1147393.678236	42.571764
3514.033569	1147110.612856	42.576768
3514.281298	1146824.021483	42.581773
3514.035305	1146533.515670	42.586778
3513.793058	1146239.297149	42.591783
3513.741854	1145966.355579	42.596788
3513.721359	1145688.750540	42.601792
3513.959245	1145404.642857	42.606797
3513.948640	1145133.642090	42.611802
3513.644075	1144846.844787	42.616807
3513.563253	1144570.044063	42.621812
3513.485501	1144295.788115	42.626816
3513.824501	1144022.018170	42.631821
3513.818476	1143741.464078	42.636826
3513.564432	1143466.435599	42.641831
3513.461548	1143198.859205	42.646836
3513.783889	1142929.397448	42.651840
3513.328501	1142635.297782	42.656845
3513.054498	1142380.700754	42.661850
3513.516031	1142094.955724	42.666855
3513.712684	1141823.276866	42.671860
3513.550441	1141563.215580	42.676864
3513.734589	1141269.598646	42.681869
3513.326833	1141008.981391	42.686874
3513.574270	1140732.969251	42.691879
3513.498294	1140454.718976	42.696884
3512.819029	1140188.128850	42.701888
3513.436023	1139920.647616	42.706893
3512.970135	1139648.681615	42.711898
3512.893914	1139371.133562	42.716903
3513.243242	1139101.662275	42.721908
3512.852798	1138856.689559	42.726912
3513.130028	1138587.868352	42.731917
3513.225943	1138319.348118	42.736922
3512.978780	1138044.701068	42.741927
3513.280232	1137783.333655	42.746932
3512.855110	1137522.547662	42.751936
3512.817707	1137247.350117	42.756941
3512.637540	1136987.636665	42.761946
3512.251456	1136745.223880	42.766951
3512.813151	1136490.870563	42.771956
3512.764495	1136230.433753	42.776960
3512.674341	1135975.308520	42.781965
3512.293980	1135710.817732	42.786970
3512.291440	1135449.195455	42.791975
3512.617502	1135201.561691	42.796980
3512.425459	1134954.286628	42.801985
3512.541875	1134677.600818	42.806989
3512.346539	1134434.006245	42.811994
3512.257482	1134176.894721	42.816999
3512.677154	1133932.320962	42.822004
3512.672491	1133675.551243	42.827009
3512.456104	1133416.428946	42.832013
3511.981180	1133177.477860	42.837018
3511.955227	1132915.354577	42.842023
3512.104329	1132668.296931	42.847028
3511.821987	1132433.556340	42.852033
3511.931413	1132189.048471	42.857037
3511.900853	1131945.027553	42.862042
3512.194683	1131690.298393	42.867047
3511.998383	1131447.517362	42.872052
3511.859731	1131196.542213	42.877057
3512.007133	1130946.173429	42.882061
3511.863206	1130702.209201	42.887066
3511.761710	1130473.435481	42.892071
3511.949182	1130227.113591	42.897076
3511.591398	1129980.109597	42.902081
3511.795824	1129730.339656	42.907085
3511.700326	1129500.002022	42.912090
3511.757710	1129261.737957	42.917095
3511.528486	1129024.366153	42.922100
3511.661997	1128791.773320	42.927105
3511.452644	1128552.095167	42.932109
3511.486712	1128321.685217	42.937114
3511.553526	1128076.329707	42.942119
3511.798324	1127842.250632	42.947124
3511.392454	1127615.781749	42.952129
3511.588474	1127363.049012	42.957133
3511.451263	1127123.960484	42.962138
3511.300776	1126894.850818	42.967143
3511.202796	1126654.212866	42.972148
3511.349851	1126426.936532	42.977153
3511.612842	1126189.167060	42.982157
3511.155634	1125968.534714	42.987162
3511.378009	1125737.030651	42.992167
3511.669972	1125491.994784	42.997172
3511.151704	1125270.011584	43.002177
3511.211754	1125033.270624	43.007181
3511.286970	1124802.987231	43.012186
3511.252841	1124569.286167	43.017191
3511.279590	1124341.464987	43.022196
3510.970015	1124117.591344	43.027201
3511.143304	1123881.637153	43.032205
3511.172850	1123645.981737	43.037210
3511.168868	1123416.317788	43.042215
3511.062983	1123195.512864	43.047220
3510.874259	1122975.283579	43.052225
3511.030418	1122738.139425	43.057229
3511.117468	1122516.417918	43.062234
3510.920515	1122289.688376	43.067239
3510.947757	1122072.242289	43.072244
3510.837140	1121842.909056	43.077249
3510.465774	1121621.416317	43.082253
3510.578938	1121397.739842	43.087258
3510.520328	1121171.701797	43.092263
3510.869561	1120947.491506	43.097268
3510.675769	1120730.693802	43.102273
3510.122801	1120510.613345	43.107277
3510.351941	1120302.870886	43.112282
3510.121649	1120086.434007	43.117287
3510.889374	1119869.824001	43.122292
3510.707220	1119656.981059	43.127297
3510.673995	1119436.961300	43.132301
3510.370177	1119222.692346	43.137306
3510.510018	1119001.768894	43.142311
3510.484746	1118783.435606	43.147316
3510.318102	1118580.454575	43.152321
3510.753330	1118362.980957	43.157325
3510.413072	1118154.867790	43.162330
3510.433990	1117941.446782	43.167335
3510.679353	1117714.355046	43.172340
3510.646202	1117497.495107	43.177345
3510.884783	1117278.389978	43.182349
3510.675554	1117066.020165	43.187354
3510.414477	1116842.596010	43.192359
3510.292592	1116616.280574	43.197364
3510.022386	1116417.809047	43.202369
3510.306061	1116200.367882	43.207373
3510.144062	1115996.239707	43.212378
3510.138378	1115783.880844	43.217383
3510.401985	1115569.372181	43.222388
3509.835641	1115367.288353	43.227393
3510.156507	1115142.553570	43.232397
3510.113243	1114944.943380	43.237402
3510.055409	1114737.032181	43.242407
3510.313243	1114525.056722	43.247412
3509.739793	1114316.737450	43.252417
3510.101439	1114109.686263	43.257421
3510.018791	1113897.837437	43.262426
3509.977060	1113698.560121	43.267431
3509.895682	1113480.210581	43.272436
3509.495304	1113280.786096	43.277441
3509.760833	1113084.296174	43.282445
3509.636902	1112887.577099	43.287450
3509.422506	1112680.756379	43.292455
3509.775585	1112476.218599	43.297460
3509.340857	1112287.635566	43.302465
3509.553376	1112085.776648	43.307469
3509.415502	1111895.795613	43.312474
3509.604608	1111697.359813	43.317479
3509.682418	1111492.257559	43.322484
3509.420953	1111300.177174	43.327489
3509.348221	1111094.893746	43.332493
3509.400679	1110918.393468	43.337498
3509.522430	1110719.646435	43.342503
3509.697695	1110518.307180	43.347508
3509.472988	1110330.384076	43.352513
3509.170260	1110124.624383	43.357517
3509.279490	1109934.056171	43.362522
3509.124884	1109746.864470	43.367527
3509.404987	1109545.948638	43.372532
3509.326413	1109358.349177	43.377537
3509.175278	1109157.394417	43.382541
3508.930772	1108967.422796	43.387546
3508.842467	1108790.971263	43.392551
3509.228855	1108590.574873	43.397556
3509.194086	1108410.188835	43.402561
3509.002022	1108213.691549	43.407565
3508.997635	1108035.674206	43.412570
3509.163378	1107851.704630	43.417575
3509.179594	1107660.784797	43.422580
3508.790067	1107476.989317	43.427585
3509.005893	1107280.581694	43.432589
3509.003092	1107103.106037	43.437594
3508.515059	1106923.031187	43.442599
3508.719609	1106742.072432	43.447604
3508.755656	1106555.120118	43.452609
3508.913708	1106367.759286	43.457613
3508.674384	1106197.740413	43.462618
3508.893589	1106010.930011	43.467623
3508.770625	1105830.090037	43.472628
3508.552600	1105639.901033	43.477633
3508.788216	1105451.445090	43.482637
3508.872047	1105282.681092	43.487642
3508.364309	1105099.110366	43.492647
3508.655930	1104917.693945	43.497652
3508.690897	1104737.937394	43.502657
3508.819487	1104543.545568	43.507661
3508.754694	1104374.968646	43.512666
3508.567170	1104193.511241	43.517671
3508.659369	1104010.759833	43.522676
3508.543562	1103824.310884	43.527681
3508.689594	1103649.276140	43.532685
3508.611744	1103470.069068	43.537690
3508.365458	1103301.775070	43.542695
3508.574827	1103121.362653	43.547700
3508.438281	1102952.275345	43.552705
3508.238197	1102771.536484	43.557709
3508.528775	1102595.297160	43.562714
3508.048771	1102434.467478	43.567719
3508.471740	1102245.677484	43.572724
3508.228865	1102090.531863	43.577729
3508.300421	1101918.128850	43.582733
3508.225696	1101738.768162	43.587738
3508.053892	1101578.626717	43.592743
3508.269825	1101401.022727	43.597748
3508.441065	1101226.383059	43.602753
3508.179956	1101054.389536	43.607757
3508.249591	1100881.953737	43.612762
3508.483732	1100706.522250	43.617767
3508.379467	1100528.751131	43.622772
3507.960193	1100368.136587	43.627777
3508.081434	1100201.883883	43.632781
3507.972874	1100023.427683	43.637786
3507.890812	1099865.323721	43.642791
3508.230348	1099691.753879	43.647796
3507.998697	1099523.530781	43.652801
3508.115726	1099369.872935	43.657805
3508.093636	1099192.522324	43.662810
3507.916482	1099036.895640	43.667815
3508.324669	1098863.957195	43.672820
3507.852479	1098693.261832	43.677825
3508.082168	1098523.592943	43.682829
3507.326471	1098362.878524	43.687834
3507.712722	1098207.804542	43.692839
3507.748870	1098045.228962	43.697844
3507.619104	1097893.673657	43.702849
3507.446720	1097720.029165	43.707853
3507.595403	1097573.679027	43.712858
3507.292736	1097420.513068	43.717863
3507.967085	1097257.330480	43.722868
3508.016271	1097102.471608	43.727873
3507.921954	1096924.675879	43.732877
3507.878256	1096778.431558	43.737882
3507.625894	1096613.469116	43.742887
3508.007691	1096443.231618	43.747892
3507.708139	1096285.345697	43.752897
3507.490438	1096123.136780	43.757901
3507.641917	1095973.203287	43.762906
3507.581984	1095809.045623	43.767911
3507.788812	1095653.736633	43.772916
3507.557453	1095500.121840	43.777921
3507.345791	1095339.227881	43.782925
3507.701147	1095197.276303	43.787930
3507.358533	1095034.002812	43.792935
3507.516795	1094867.579926	43.797940
3507.554835	1094726.338069	43.802945
3507.428090	1094559.091436	43.807949
3507.282149	1094410.790417	43.812954
3507.225452	1094270.509221	43.817959
3507.548892	1094105.949671	43.822964
3507.267980	1093956.127223	43.827969
3507.012964	1093803.042373	43.832973
3507.152071	1093662.043228	43.837978
3506.870147	1093514.410009	43.842983
3507.064424	1093359.802974	43.847988
3506.859746	1093224.304719	43.852993
3507.173097	1093075.030033	43.857997
3506.963033	1092929.379121	43.863002
3507.014017	1092786.840178	43.868007
3507.302236	1092641.960988	43.873012
3506.992012	1092496.985031	43.878017
3507.085318	1092348.205214	43.883021
3506.669815	1092199.888047	43.888026
3506.825044	1092053.100344	43.893031
3507.065539	1091910.219927	43.898036
3506.741930	1091768.194584	43.903041
3506.877346	1091617.089970	43.908045
3506.888532	1091490.704249	43.913050
3506.997806	1091351.086092	43.918055
3507.042258	1091206.017185	43.923060
3506.936131	1091055.606968	43.928065
3506.425355	1090910.047060	43.933069
3506.743323	1090771.432935	43.938074
3506.459714	1090636.170240	43.943079
3506.988315	1090494.641509	43.948084
3506.340861	1090352.440880	43.953089
3506.504924	1090210.581713	43.958093
3506.564916	1090080.228553	43.963098
3506.414508	1089956.036424	43.968103
3506.610285	1089806.020702	43.973108
3506.414907	1089686.522842	43.978113
3506.343029	1089540.470770	43.983117
3506.484261	1089411.620666	43.988122
3506.384920	1089278.400993	43.993127
3506.587201	1089148.289373	43.998132
3506.551039	1089007.964356	44.003137
3506.607765	1088878.636569	44.008141
3506.777452	1088750.819816	44.013146
3506.363052	1088612.941752	44.018151
3506.613190	1088464.604362	44.023156
3506.589755	1088340.641755	44.028161
3506.833068	1088202.644949	44.033165
3506.486692	1088057.843654	44.038170
3506.433428	1087925.445455	44.043175
3506.577698	1087787.741850	44.048180
3506.571339	1087659.161908	44.053185
3506.591843	1087517.351826	44.058189
3506.623656	1087398.628530	44.063194
3506.242472	1087250.649425	44.068199
3506.535247	1087108.017248	44.073204
3506.492632	1086977.798147	44.078209
3506.144050	1086855.963379	44.083213
3506.389795	1086721.474200	44.088218
3506.284590	1086591.256144	44.093223
3506.659386	1086458.751704	44.098228
3506.162543	1086324.470839	44.103233
3506.532093	1086205.474177	44.108237
3506.384782	1086071.033644	44.113242
3506.450389	1085935.117051	44.118247
3506.347452	1085802.771153	44.123252
3505.926843	1085685.426796	44.128257
3506.071119	1085545.749406	44.133261
3506.149205	1085433.110035	44.138266
3506.071625	1085297.009368	44.143271
3506.291240	1085157.309597	44.148276
3506.095695	1085044.611388	44.153281
3505.962618	1084906.592886	44.158285
3506.087359	1084792.590491	44.163290
3506.001908	1084675.936060	44.168295
3506.423588	1084533.215119	44.173300
3505.985865	1084418.914052	44.178305
3506.094747	1084289.372571	44.183309
3506.177088	1084163.092152	44.188314
3505.958921	1084045.103791	44.193319
3506.242663	1083923.674413	44.198324
3505.861082	1083795.927800	44.203329
3505.770210	1083672.445106	44.208333
3506.207668	1083556.831172	44.213338
3505.728770	1083416.626436	44.218343
3506.205530	1083301.959508	44.223348
3505.950428	1083184.342128	44.228353
3505.654789	1083048.029322	44.233357
3505.821131	1082937.049858	44.238362
3505.722343	1082822.947123	44.243367
3505.969769	1082691.139105	44.248372
3505.574906	1082578.614436	44.253377
3505.597299	1082455.852717	44.258381
3505.851729	1082338.612674	44.263386
3505.520720	1082230.386141	44.268391
3505.838995	1082099.798973	44.273396
3505.674793	1081994.225810	44.278401
3505.495001	1081880.883986	44.283405
3505.655841	1081758.947002	44.288410
3505.308735	1081647.642157	44.293415
3505.634820	1081534.977180	44.298420
3505.310111	1081421.457817	44.303425
3505.734597	1081306.853439	44.308429
3505.562364	1081183.039905	44.313434
3505.526243	1081066.204051	44.318439
3505.607958	1080961.145944	44.323444
3505.396157	1080854.119541	44.328449
3505.525090	1080730.821733	44.333453
3505.793195	1080622.944263	44.338458
3505.505643	1080504.794650	44.343463
3505.683806	1080380.809239	44.348468
3505.660786	1080279.113218	44.353473
3505.013045	1080170.418187	44.358477
3505.763274	1080049.497245	44.363482
3505.477918	1079949.277498	44.368487
3505.921527	1079831.856428	44.373492
3505.464121	1079716.980075	44.378497
3505.278748	1079601.960541	44.383501
3505.529934	1079488.977757	44.388506
3505.204566	1079372.537069	44.393511
3505.434634	1079263.103606	44.398516
3505.393542	1079165.900009	44.403521
3505.376043	1079061.397419	44.408525
3505.279129	1078949.036577	44.413530
3505.314699	1078839.338746	44.418535
3505.437202	1078736.246411	44.423540
3505.351416	1078624.356905	44.428545
3505.449044	1078508.595889	44.433549
3505.658038	1078393.485917	44.438554
3505.164925	1078278.105234	44.443559
3505.583614	1078165.739322	44.448564
3505.173329	1078071.360482	44.453569
3504.939755	1077954.490463	44.458573
3505.146154	1077859.334494	44.463578
3505.116545	1077762.391958	44.468583
3505.522169	1077646.273962	44.473588
3504.997895	1077537.890046	44.478593
3505.153272	1077433.711778	44.483597
3504.827475	1077324.138997	44.488602
3505.189059	1077227.986507	44.493607
3505.330644	1077117.564623	44.498612
3505.197867	1077018.993881	44.503617
3504.967913	1076921.493398	44.508621
3505.190756	1076817.772286	44.513626
3505.059818	1076702.682649	44.518631
3504.893739	1076588.844491	44.523636
3504.843952	1076498.603462	44.528641
3505.037412	1076388.062273	44.533645
3504.899571	1076293.895849	44.538650
3504.687249	1076195.515368	44.543655
3504.599099	1076095.384346	44.548660
3504.747523	1076003.374171	44.553665
3504.824484	1075915.983218	44.558669
3505.079195	1075812.045723	44.563674
3504.698959	1075708.114799	44.568679
3504.892278	1075623.292663	44.573684
3504.779048	1075512.112082	44.578689
3504.691733	1075412.352514	44.583693
3505.046788	1075318.568246	44.588698
3504.608079	1075227.698054	44.593703
3504.811596	1075128.077463	44.598708
3504.756470	1075026.961072	44.603713
3504.969511	1074925.990721	44.608717
3504.592408	1074832.030575	44.613722
3504.839381	1074737.197698	44.618727
3504.763538	1074634.444751	44.623732
3504.887843	1074543.662539	44.628737
3504.786924	1074438.028681	44.633741
3504.576889	1074344.032626	44.638746
3504.295466	1074253.888714	44.643751
3504.607795	1074158.458737	44.648756
3504.747064	1074070.835917	44.653761
3504.470530	1073978.189268	44.658765
3504.468695	1073879.060016	44.663770
3504.494640	1073793.756779	44.668775
3504.656208	1073689.025799	44.673780
3504.541782	1073604.511208	44.678785
3504.535224	1073516.135027	44.683789
3504.761431	1073409.274659	44.688794
3504.337990	1073327.976827	44.693799
3504.718006	1073239.532510	44.698804
3504.504773	1073144.171400	44.703809
3504.105545	1073059.214939	44.708813
3504.329641	1072975.499513	44.713818
3504.248781	1072873.482875	44.718823
3504.432441	1072790.539874	44.723828
3504.520996	1072713.375908	44.728833
3504.509655	1072615.570403	44.733837
3504.824635	1072527.893932	44.738842
3504.243838	1072439.114523	44.743847
3504.521764	1072340.872139	44.748852
3504.582233	1072253.617527	44.753857
3504.669403	1072166.453213	44.758861
3504.690434	1072072.572225	44.763866
3504.446484	1071988.438347	44.768871
3504.559906	1071888.965781	44.773876
3504.398627	1071809.716207	44.778881
3504.352134	1071722.662933	44.783885
3504.555350	1071626.438019	44.788890
3504.480932	1071548.996191	44.793895
3504.611926	1071439.902811	44.798900
3504.285821	1071350.102778	44.803905
3504.395837	1071253.502257	44.808909
3504.609940	1071157.459517	44.813914
3504.355442	1071085.710950	44.818919
3504.141605	1070997.808758	44.823924
3504.502465	1070922.689062	44.828929
3504.395507	1070832.748338	44.833933
3504.528641	1070746.899396	44.838938
3504.108171	1070653.259004	44.843943
3504.233749	1070559.238732	44.848948
3504.225376	1070484.077719	44.853953
3504.031570	1070402.121866	44.858957
3504.318753	1070314.702897	44.863962
3504.172291	1070227.065591	44.868967
3504.243879	1070139.967705	44.873972
3504.027300	1070060.798038	44.878977
3504.017474	1069992.743668	44.883981
3504.156733	1069897.940796	44.888986
3503.880689	1069824.833478	44.893991
3503.954111	1069743.785039	44.898996
3503.964446	1069664.476142	44.904001
3503.735615	1069564.633202	44.909005
3504.307879	1069483.114222	44.914010
3504.075754	1069404.610566	44.919015
3504.311911	1069329.105030	44.924020
3504.316053	1069248.060671	44.929025
3504.095038	1069159.264904	44.934029
3504.450668	1069076.045045	44.939034
3504.129965	1068998.992279	44.944039
3504.304698	1068915.511349	44.949044
3504.412306	1068827.136797	44.954049
3504.375430	1068735.323329	44.959053
3504.112155	1068651.045189	44.964058
3504.033830	1068574.619573	44.969063
3503.710387	1068472.945476	44.974068
3503.596529	1068405.561589	44.979073
3503.531450	1068343.072684	44.984077
3504.276940	1068266.891715	44.989082
3504.057778	1068191.637817	44.994087
3503.928176	1068102.329085	44.999092
3504.357353	1068028.985494	45.004097
3504.007638	1067954.038313	45.009101
3504.160962	1067865.063763	45.014106
3503.691892	1067793.403554	45.019111
3504.024350	1067718.148469	45.024116
3503.971148	1067639.301559	45.029121
3503.871109	1067560.461228	45.034125
3504.288444	1067482.496244	45.039130
3503.986206	1067409.841853	45.044135
3504.068272	1067322.889819	45.049140
3503.967627	1067243.660347	45.054145
3503.930591	1067159.610531	45.059149
3503.877965	1067083.159893	45.064154
3503.549793	1067022.334257	45.069159
3503.747906	1066941.031493	45.074164
3503.803327	1066861.097544	45.079169
3503.642748	1066794.855713	45.084173
3503.911936	1066713.441692	45.089178
3503.720557	1066650.377205	45.094183
3503.767119	1066559.667767	45.099188
3503.968461	1066488.841935	45.104193
3504.011405	1066415.059463	45.109197
3504.143098	1066334.335779	45.114202
3503.977115	1066255.679933	45.119207
3503.611918	1066177.055769	45.124212
3504.076036	1066099.159631	45.129217
3503.574380	1066029.790361	45.134221
3503.993047	1065958.633314	45.139226
3503.880226	1065884.773172	45.144231
3503.629070	1065805.355323	45.149236
3503.458711	1065739.871949	45.154241
3503.651947	1065664.323043	45.159245
3503.985730	1065588.365143	45.164250
3503.502894	1065523.507863	45.169255
3503.901152	1065439.456211	45.174260
3503.737046	1065356.650366	45.179265
3503.397298	1065290.804707	45.184269
3503.848422	1065215.591986	45.189274
3503.777443	1065142.099793	45.194279
3503.498123	1065058.923592	45.199284
3503.419688	1064999.669980	45.204289
3503.583280	1064939.606161	45.209293
3503.674243	1064864.351737	45.214298
3503.333598	1064802.156520	45.219303
3503.759624	1064730.308846	45.224308
3503.776076	1064652.850803	45.229313
3503.425032	1064595.946975	45.234317
3503.691205	1064518.445908	45.239322
3503.478348	1064460.459487	45.244327
3503.445644	1064380.311485	45.249332
3503.395654	1064318.832707	45.254337
3503.494506	1064245.685443	45.259341
3503.683095	1064170.309208	45.264346
3503.608250	1064104.309457	45.269351
3503.696038	1064016.534280	45.274356
3503.701292	1063957.351869	45.279361
3503.635194	1063895.101157	45.284365
3503.776285	1063831.853288	45.289370
3503.531975	1063767.898294	45.294375
3503.175908	1063690.488033	45.299380
3503.385776	1063623.088314	45.304385
3503.464533	1063557.826591	45.309389
3503.631798	1063483.695542	45.314394
3503.471815	1063426.363165	45.319399
3503.798212	1063355.380094	45.324404
3503.818748	1063285.793876	45.329409
3503.316512	1063216.004145	45.334413
3503.625185	1063149.641030	45.339418
3503.435822	1063074.696998	45.344423
3503.646026	1063006.134709	45.349428
3503.809455	1062945.664137	45.354433
3503.161911	1062885.133965	45.359437
3503.238711	1062809.757486	45.364442
3503.363839	1062744.863477	45.369447
3503.485723	1062670.825195	45.374452
3503.458422	1062608.649772	45.379457
3503.384846	1062543.016073	45.384461
3503.460021	1062472.062979	45.389466
3503.403006	1062422.211178	45.394471
3503.696763	1062341.498383	45.399476
3503.346638	1062287.458240	45.404481
3503.321448	1062224.700567	45.409485
3503.691064	1062145.127529	45.414490
3503.370007	1062083.668386	45.419495
3503.340414	1062019.080087	45.424500
3503.230101	1061954.504323	45.429505
3503.594768	1061893.218911	45.434509
3503.538454	1061824.974595	45.439514
3503.451375	1061762.799452	45.444519
3503.553383	1061691.735604	45.449524
3503.200791	1061633.260995	45.454529
3503.378148	1061565.745147	45.459533
3503.362063	1061490.173335	45.464538
3503.153399	1061442.840749	45.469543
3503.210887	1061368.602994	45.474548
3503.413995	1061316.676532	45.479553
3503.389506	1061243.702193	45.484557
3503.398037	1061173.994946	45.489562
3503.082135	1061123.692613	45.494567
3503.451714	1061054.309508	45.499572
3503.721520	1060997.458695	45.504577
3503.214054	1060923.500545	45.509581
3503.511973	1060862.310936	45.514586
3503.449392	1060799.639446	45.519591
3503.189307	1060728.526507	45.524596
3503.100377	1060657.384459	45.529601
3502.937059	1060606.089375	45.534605
3503.205507	1060550.967382	45.539610
3503.131214	1060483.479704	45.544615
3503.086191	1060424.941585	45.549620
3503.017937	1060363.999330	45.554625
3503.076135	1060302.746691	45.559629
3503.448467	1060242.597182	45.564634
3503.192921	1060185.535623	45.569639
3503.227625	1060118.025512	45.574644
3503.082873	1060065.085262	45.579649
3502.901281	1059994.720297	45.584653
3502.970739	1059937.987843	45.589658
3502.849767	1059900.353927	45.594663
3503.118512	1059830.394201	45.599668
3502.932764	1059781.695301	45.604673
3502.515067	1059728.026330	45.609677
3502.906343	1059668.926789	45.614682
3502.948945	1059618.551639	45.619687
3502.875198	1059559.720128	45.624692
3503.092963	1059512.397001	45.629697
3502.912060	1059457.338072	45.634701
3503.176173	1059401.916368	45.639706
3502.958054	1059339.157550	45.644711
3503.278959	1059280.739618	45.649716
3502.941179	1059221.081161	45.654721
3502.822400	1059164.756997	45.659725
3503.008068	1059108.189484	45.664730
3503.237987	1059059.126783	45.669735
3502.953626	1058994.063348	45.674740
3503.310828	1058938.525335	45.679745
3502.967478	1058878.478807	45.684749
3503.274786	1058823.333129	45.689754
3503.115129	1058766.818986	45.694759
3502.682708	1058717.477043	45.699764
3502.956707	1058658.193336	45.704769
3502.972517	1058604.923626	45.709773
3502.904908	1058535.484476	45.714778
3502.764130	1058481.757736	45.719783
3502.546602	1058431.510897	45.724788
3502.511968	1058383.063713	45.729793
3502.760646	1058330.427293	45.734797
3503.034024	1058283.855091	45.739802
3502.794168	1058230.816530	45.744807
3502.928513	1058173.862556	45.749812
3503.069974	1058112.668175	45.754817
3502.659760	1058043.086577	45.759821
3502.819452	1057925.820370	45.764826
3502.815987	1057758.867789	45.769831
3502.616108	1057517.084243	45.774836
3502.841532	1057223.384815	45.779841
3502.464496	1056863.862713	45.784845
3502.858617	1056435.869758	45.789850
3502.163605	1055963.692727	45.794855
3502.525476	1055419.113048	45.799860
3502.499277	1054807.263252	45.804865
3502.096216	1054123.588196	45.809869
3502.206565	1053376.784820	45.814874
3502.191461	1052565.679220	45.819879
3502.158501	1051679.616423	45.824884
3501.785074	1050714.658630	45.829889
3501.489773	1049685.939519	45.834893
3501.830240	1048581.655389	45.839898
3501.071450	1047409.672029	45.844903
3501.119640	1046148.586496	45.849908
3500.999576	1044806.320641	45.854913
3500.446598	1043403.626110	45.859917
3500.337059	1041901.570225	45.864922
3500.346573	1040335.207660	45.869927
3500.205525	1038682.777780	45.874932
3499.943271	1036953.096033	45.879937
3499.380121	1035116.326626	45.884941
3499.285269	1033217.717998	45.889946
3498.961792	1031248.997709	45.894951
3498.404279	1029176.200474	45.899956
3498.236568	1027020.227138	45.904961
3497.750726	1024793.116395	45.909965
3497.852422	1022461.768314	45.914970
3497.399525	1020062.518393	45.919975
3496.972404	1017574.225225	45.924980
3496.542397	1014990.951882	45.929985
3496.317597	1012330.212325	45.934989
3495.703283	1009579.363933	45.939994
3495.194036	1006758.612532	45.944999
3494.829060	1003850.729076	45.950004
3494.345245	1000841.804796	45.955009
3493.698921	997773.172025	45.960013
3493.317611	994605.108763	45.965018
3492.908946	991373.278488	45.970023
3492.156855	988047.291545	45.975028
3492.055201	984623.016436	45.980033
3491.276349	981138.295170	45.985037
3491.359141	977556.903038	45.990042
3490.864094	973895.622336	45.995047
3490.030312	970147.513816	46.000052
3489.629778	966295.443962	46.005057
3488.509647	962370.460758	46.010061
3488.358979	958359.592465	46.015066
3487.354510	954301.706114	46.020071
3486.727451	950231.307470	46.025076
3486.240279	946083.040589	46.030081
3485.077725	941855.442680	46.035085
3485.039941	937532.703442	46.040090
3483.889893	933148.114784	46.045095
3483.040099	928667.880631	46.050100
3482.076120	924116.966585	46.055105
3481.496118	919483.403834	46.060109
3480.871337	914762.561666	46.065114
3479.301656	909966.360329	46.070119
3478.634309	905085.751420	46.075124
3478.260285	900139.881561	46.080129
3476.875349	895089.682249	46.085133
3475.902131	889964.785068	46.090138
3474.998528	884767.227804	46.095143
3474.233718	879480.084419	46.100148
3473.391270	874116.302294	46.105153
3472.203103	868674.317189	46.110157
3471.396392	863136.454035	46.115162
3470.061798	857536.035032	46.120167
3468.991870	851834.060198	46.125172
3468.256687	846060.229950	46.130177
3466.832526	840206.972423	46.135181
3465.903515	834267.839345	46.140186
3464.699270	828248.706695	46.145191
3463.585995	822139.632517	46.150196
3462.380135	815956.095425	46.155201
3461.280861	809687.056117	46.160205
3460.361936	803340.295549	46.165210
3458.663142	796908.673527	46.170215
3457.609491	790393.135481	46.175220
3456.514446	783805.312685	46.180225
3455.197735	777136.168271	46.185229
3453.925714	770368.528829	46.190234
3452.542538	763543.882128	46.195239
3451.343213	756617.937968	46.200244
3450.088102	749615.768396	46.205249
3448.333716	742541.206477	46.210253
3447.187371	735365.965406	46.215258
3445.826562	728121.143104	46.220263
3444.232938	720788.870515	46.225268
3442.913434	713380.171448	46.230273
3441.309641	705885.969451	46.235277
3440.004626	698330.536759	46.240282
3438.614144	690684.844811	46.245287
3437.395050	682958.366333	46.250292
3436.333489	675144.654343	46.255297
3434.339339	667258.228237	46.260301
3432.887091	659277.785415	46.265306
3431.011991	651224.789790	46.270311
3429.204112	643087.631487	46.275316
3427.909626	634891.416318	46.280321
3425.927714	626606.454231	46.285325
3424.344738	618246.857218	46.290330
3422.700927	609823.480276	46.295335
3421.043123	601332.924678	46.300340
3419.219682	592743.231636	46.305345
3417.236867	584093.575847	46.310349
3415.524244	575355.759800	46.315354
3413.526387	566555.197143	46.320359
3411.581081	557677.428205	46.325364
3410.193462	548725.175960	46.330369
3407.898157	539696.356864	46.335373
3406.112938	530616.884300	46.340378
3403.894693	521446.205713	46.345383
3401.867262	512216.601281	46.350388
3400.024960	502911.537233	46.355393
3397.565815	493546.304740	46.360397
3395.797362	484110.778505	46.365402
3393.690695	474614.755144	46.370407
3391.390839	465042.425866	46.375412
3388.834518	455411.758631	46.380417
3386.796330	445711.865391	46.385421
3384.297566	435950.808973	46.390426
3382.219066	426137.331733	46.395431
3379.583093	416247.518611	46.400436
3377.380083	406286.999212	46.405441
3374.541201	396297.309887	46.410445
3372.480778	386220.430272	46.415450
3369.790828	376125.389104	46.420455
3367.237926	365955.073702	46.425460
3364.833433	355734.637205	46.430465
3362.105730	345471.228312	46.435469
3359.698780	335128.354459	46.440474
3356.480859	324754.715216	46.445479
3353.826115	314334.277358	46.450484
3351.183868	303851.270427	46.455489
3347.957377	293339.996374	46.460493
3344.990904	282778.385059	46.465498
3342.064405	272179.280335	46.470503
3339.083351	261539.596619	46.475508
3335.776384	250858.142860	46.480513
3332.338676	240152.732869	46.485517
3329.414548	229392.826560	46.490522
3326.275552	218542.065807	46.495527
3322.202497	207737.791771	46.500532
3319.045607	196919.419198	46.505537
3315.368767	186073.516284	46.510541
3311.533490	175210.759227	46.515546
3307.270191	164321.609837	46.520551
3303.529409	153441.167948	46.525556
3299.208526	142541.577470	46.530561
3294.508387	131664.521612	46.535565
3290.285694	120777.457179	46.540570
3285.169342	109910.911502	46.545575
3280.562906	99048.315461	46.550580
3275.069282	88211.804192	46.555585
3269.480245	77413.333516	46.560589
3263.859188	66627.350047	46.565594
3256.836331	55939.805294	46.570599
3248.188176	45348.344445	46.575604
3238.377563	34864.018922	46.580609
3217.570966	24805.006366	46.585613
3184.173108	15312.149858	46.590618
3137.654185	6619.689913	46.595623
3009.674871	851.135812	46.600628
2741.615438	456.878047	46.605633
2578.953210	453.719636	46.610637
2550.707006	435.961397	46.615642
2615.360335	421.049453	46.620647
2716.799283	406.415846	46.625652
2807.831565	401.383856	46.630657
2865.921759	410.484905	46.635661
2890.352287	405.845421	46.640666
2889.540800	407.954022	46.645671
2876.495170	400.259122	46.650676
2861.378846	385.145027	46.655681
2848.809213	396.335667	46.660685
2841.060368	388.033921	46.665690
2837.435682	406.538671	46.670695
2835.672313	380.811605	46.675700
2835.672020	377.958131	46.680705
2834.970077	370.798458	46.685709
2833.511868	368.707333	46.690714
2830.868832	377.431720	46.695719
2827.682595	383.143642	46.700724
2824.714747	371.557785	46.705729
2821.152608	381.970499	46.710733
2818.152340	373.388812	46.715738
2815.206547	371.957000	46.720743
2811.618865	363.703812	46.725748
2808.795919	374.842830	46.730753
2805.839739	374.755672	46.735757
2802.782470	364.912575	46.740762
2799.648666	358.442307	46.745767
2796.290892	359.746440	46.750772
2793.153340	356.356709	46.755777
2789.556858	365.631241	46.760781
2786.480175	365.793042	46.765786
2783.502357	361.839292	46.770791
2780.266780	349.510813	46.775796
2776.957533	352.306855	46.780801
2773.249997	358.411557	46.785805
2769.998877	345.387247	46.790810
2766.601589	355.082079	46.795815
2763.186577	353.417861	46.800820
2760.196146	343.152671	46.805825
2756.591543	361.284605	46.810829
2753.621847	353.516388	46.815834
2750.519587	351.106159	46.820839
2746.566481	346.721863	46.825844
2743.421025	344.043207	46.830849
2739.678620	349.594770	46.835853
2736.777162	337.827754	46.840858
2733.195877	331.517236	46.845863
2729.589066	340.291703	46.850868
2726.858427	328.771595	46.855873
2722.954516	344.709185	46.860877
2719.526216	329.305292	46.865882
2716.193932	338.734481	46.870887
2712.618163	331.952761	46.875892
2709.060612	337.421271	46.880897
2705.851707	340.458786	46.885901
2702.664327	331.895005	46.890906
2699.689723	343.704156	46.895911
2695.617754	331.334375	46.900916
2692.058674	330.675395	46.905921
2688.734178	335.355687	46.910925
2685.382102	332.265979	46.915930
2681.742503	337.731059	46.920935
2678.979300	335.541400	46.925940
2675.610762	329.911402	46.930945
2671.891208	329.126562	46.935949
2668.172352	319.768332	46.940954
2664.898490	328.337074	46.945959
2660.802565	330.352743	46.950964
2657.564038	325.640939	46.955969
2654.042486	320.455185	46.960973
2651.434429	326.960332	46.965978
2647.863665	329.192004	46.970983
2643.629487	332.477415	46.975988
2640.672245	316.447575	46.980993
2637.269905	314.558067	46.985997
2633.481586	330.858616	46.991002
2629.756901	325.224224	46.996007
2626.416691	325.672830	47.001012
2623.580918	318.119094	47.006017
2619.967364	321.990719	47.011021
2616.832643	316.743473	47.016026
2613.413010	317.779269	47.021031
2609.398670	325.975253	47.026036
2605.562200	318.358428	47.031041
2601.872723	318.180441	47.036045
2598.351820	320.787198	47.041050
2595.471853	321.067783	47.046055
2592.304870	327.044646	47.051060
2589.188483	322.357230	47.056065
2585.642230	321.809346	47.061069
2582.107452	309.650015	47.066074
2578.720388	321.873085	47.071079
2574.631638	309.254295	47.076084
2571.684132	311.962154	47.081089
2567.855289	318.992015	47.086093
2563.881250	296.926099	47.091098
2560.583177	306.945966	47.096103
2557.323741	307.636017	47.101108
2554.100816	305.865346	47.106113
2550.542790	311.581029	47.111117
2546.846079	310.361449	47.116122
2543.098170	312.004580	47.121127
2539.743863	316.661820	47.126132
2536.957708	309.650259	47.131137
2533.411998	316.644694	47.136141
2529.530041	309.266869	47.141146
2526.200386	301.980200	47.146151
2522.890112	305.942046	47.151156
2518.941647	304.832166	47.156161
2515.465459	307.984954	47.161165
2512.045865	307.263103	47.166170
2508.806392	301.337155	47.171175
2505.212228	304.982662	47.176180
2501.412861	302.200820	47.181185
2497.699929	313.879878	47.186189
2494.707843	307.087869	47.191194
2491.691582	300.448924	47.196199
2488.243477	302.164879	47.201204
2484.591938	293.011042	47.206209
2480.671874	314.903554	47.211213
2477.388480	304.057209	47.216218
2474.114988	300.333008	47.221223
2470.124877	302.441721	47.226228
2466.777482	290.718126	47.231233
2462.963815	299.183453	47.236237
2459.474198	298.635071	47.241242
2456.549245	288.594374	47.246247
2453.041837	285.850347	47.251252
2449.803246	284.978315	47.256257
2445.844310	301.797851	47.261261
2442.468221	290.532925	47.266266
2439.267408	295.159263	47.271271
2435.233282	294.263336	47.276276
2431.994612	292.757548	47.281281
2428.413594	292.787785	47.286285
2425.176243	289.379865	47.291290
2421.846516	298.592646	47.296295
2418.092663	293.056029	47.301300
2414.809603	283.431749	47.306305
2410.832432	286.541307	47.311309
2407.289028	298.391027	47.316314
2403.453078	291.807487	47.321319
2400.361525	289.432452	47.326324
2397.296927	285.090579	47.331329
2393.586172	291.859614	47.336333
2390.190116	286.995752	47.341338
2386.708051	282.465531	47.346343
2383.135970	289.854157	47.351348
2379.667239	282.002411	47.356353
2376.088128	283.724036	47.361357
2372.493452	279.165729	47.366362
2368.913976	278.729682	47.371367
2365.318693	287.770211	47.376372
2362.169111	291.417931	47.381377
2358.887736	287.115673	47.386381
2355.380798	277.337250	47.391386
2351.964629	275.648561	47.396391
2348.040465	287.903230	47.401396
2344.499321	282.241307	47.406401
2340.961620	291.706345	47.411405
2337.605304	284.342293	47.416410
2334.157902	288.845466	47.421415
2330.336850	282.187792	47.426420
2327.275723	276.256210	47.431425
2323.575738	283.771612	47.436429
2320.390571	279.320419	47.441434
2317.022253	281.631314	47.446439
2313.227207	281.437138	47.451444
2309.724026	279.320242	47.456449
2306.000824	287.561555	47.461453
2302.800022	278.106584	47.466458
2299.023071	284.770355	47.471463
2295.539819	287.427263	47.476468
2292.323775	278.669556	47.481473
2289.107450	280.299324	47.486477
2285.595832	272.462107	47.491482
2281.753628	274.012783	47.496487
2277.908991	288.597078	47.501492
2274.476433	271.455780	47.506497
2271.118258	272.755165	47.511501
2268.309168	281.410541	47.516506
2264.718084	282.140219	47.521511
2260.800944	292.332620	47.526516
2257.417683	278.269097	47.531521
2253.613598	287.119167	47.536525
2250.255618	279.705616	47.541530
2246.892836	274.885079	47.546535
2243.220054	278.216908	47.551540
2239.842004	275.677677	47.556545
2236.257791	289.320663	47.561549
2232.547066	280.617444	47.566554
2229.617914	262.135968	47.571559
2225.450784	282.304972	47.576564
2222.079714	275.421511	47.581569
2219.033705	270.623230	47.586573
2215.071185	279.808043	47.591578
2211.698887	273.691555	47.596583
2208.258514	274.603977	47.601588
2204.749011	265.372829	47.606593
2201.320136	264.510588	47.611597
2198.290679	274.711385	47.616602
2194.635566	265.497847	47.621607
2190.835134	274.706939	47.626612
2187.587183	273.328977	47.631617
2183.832163	268.801067	47.636621
2179.984792	285.223037	47.641626
2176.478783	272.635303	47.646631
2173.182149	266.194503	47.651636
2169.917055	269.048114	47.656641
2166.695840	270.304433	47.661645
2162.954003	274.024953	47.666650
2159.572077	272.273585	47.671655
2155.450136	268.274340	47.676660
2152.497493	265.501707	47.681665
2148.871356	258.680688	47.686669
2145.167677	269.110206	47.691674
2141.753710	272.228615	47.696679
2138.121969	271.787587	47.701684
2134.996735	266.681087	47.706689
2131.606140	273.291655	47.711693
2127.818652	265.998744	47.716698
2124.171426	269.575421	47.721703
2120.877028	270.489357	47.726708
2117.494008	266.737524	47.731713
2113.822372	269.471854	47.736717
2110.226467	271.522332	47.741722
2107.327307	267.973542	47.746727
2103.399320	264.486923	47.751732
2100.004563	263.230493	47.756737
2096.359503	264.470233	47.761741
2092.455786	258.362546	47.766746
2089.373037	264.804452	47.771751
2085.427313	259.007364	47.776756
2082.277708	255.778802	47.781761
2079.029901	268.285151	47.786765
2075.793234	262.219174	47.791770
2072.212234	262.284799	47.796775
2068.023649	268.637524	47.801780
2064.778774	266.970145	47.806785
2061.282389	263.100106	47.811789
2057.543255	266.210527	47.816794
2054.227228	262.306893	47.821799
2050.578405	262.600663	47.826804
2047.479410	253.435478	47.831809
2044.151343	267.035269	47.836813
2040.610678	257.721063	47.841818
2037.028126	259.427329	47.846823
2033.174186	266.448417	47.851828
2029.506877	251.887229	47.856833
2026.338996	259.919735	47.861837
2022.792715	263.024602	47.866842
2019.474849	260.420698	47.871847
2015.835577	261.747721	47.876852
2012.391811	248.900535	47.881857
2008.895069	263.110234	47.886861
2005.477568	257.988970	47.891866
2001.636217	258.607041	47.896871
1998.055181	263.640178	47.901876
1994.939116	253.947161	47.906881
1991.478568	264.975135	47.911885
1987.590331	259.484324	47.916890
1984.494314	261.182273	47.921895
1980.959169	261.597121	47.926900
1977.972501	253.597225	47.931905
1974.112149	257.603754	47.936909
1970.125601	256.399038	47.941914
1966.390492	253.241864	47.946919
1963.007893	248.508114	47.951924
1960.079657	244.072827	47.956929
1956.635546	246.876932	47.961933
1953.009496	248.502607	47.966938
1949.831922	248.168181	47.971943
1945.777898	255.373750	47.976948
1942.409729	249.325594	47.981953
1938.613303	248.920024	47.986957
1935.114821	259.225199	47.991962
1932.123515	245.154662	47.996967
1928.087097	251.518160	48.001972
1924.942454	248.011038	48.006977
1921.284894	248.935052	48.011981
1917.856293	248.196716	48.016986
1914.454392	247.860048	48.021991
1910.621869	253.372251	48.026996
1907.557707	244.201102	48.032001
1903.993823	248.882300	48.037005
1900.246203	250.063089	48.042010
1896.845192	247.818657	48.047015
1893.296196	253.984456	48.052020
1890.012196	246.479589	48.057025
1886.442206	248.081644	48.062029
1882.713891	263.343483	48.067034
1879.300969	247.203556	48.072039
1875.752971	246.653838	48.077044
1872.727296	239.453341	48.082049
1868.727113	246.107943	48.087053
1865.214965	254.444730	48.092058
1861.702790	243.620239	48.097063
1858.042429	247.152733	48.102068
1854.839347	242.392383	48.107073
1851.236268	243.432145	48.112077
1847.688767	239.303792	48.117082
1844.409339	241.922234	48.122087
1840.701024	253.037204	48.127092
1837.242542	245.625773	48.132097
1833.991364	248.815912	48.137101
1830.517501	237.979204	48.142106
1826.974155	232.772059	48.147111
1823.262439	242.192968	48.152116
1819.686358	245.988996	48.157121
1816.082098	249.860512	48.162125
1812.477820	239.352646	48.167130
1809.360079	233.113784	48.172135
1805.605141	248.368091	48.177140
1801.909260	232.379392	48.182145
1798.720334	244.124826	48.187149
1795.379560	235.681589	48.192154
1792.250609	231.915930	48.197159
1788.630904	246.460787	48.202164
1784.473087	237.360544	48.207169
1781.092226	232.947142	48.212173
1777.715998	241.765074	48.217178
1774.523043	236.877801	48.222183
1770.902712	245.487596	48.227188
1767.403191	246.112825	48.232193
1763.576378	246.877396	48.237197
1759.825132	247.856115	48.242202
1756.722616	236.703449	48.247207
1753.150038	236.234308	48.252212
1749.994060	239.676131	48.257217
1746.206870	244.085054	48.262221
1742.502295	248.504321	48.267226
1739.175025	237.213042	48.272231
1735.555964	240.962728	48.277236
1732.656872	233.621845	48.282241
1728.980406	247.275751	48.287245
1725.344616	242.195887	48.292250
1721.945196	229.918027	48.297255
1718.375473	242.067667	48.302260
1714.760198	233.903387	48.307265
1711.230626	234.637487	48.312269
1707.828379	248.760253	48.317274
1704.046177	241.392152	48.322279
1700.728030	238.945910	48.327284
1696.941734	240.262817	48.332289
1693.462777	237.933581	48.337293
1690.169706	238.028639	48.342298
1686.836610	226.217356	48.347303
1683.192837	234.944899	48.352308
1679.777198	234.468348	48.357313
1676.384018	234.729100	48.362317
1672.624078	228.140879	48.367322
1669.035169	226.197888	48.372327
1665.353619	234.933645	48.377332
1662.376436	233.520720	48.382337
1659.101816	244.667782	48.387341
1655.758519	226.582967	48.392346
1651.984406	232.695343	48.397351
1647.958826	231.338515	48.402356
1644.635056	226.894750	48.407361
1640.933024	241.956090	48.412365
1637.114646	237.513538	48.417370
1634.246331	230.334552	48.422375
1630.573540	238.453858	48.427380
1627.234541	235.382356	48.432385
1624.082388	231.980998	48.437389
1619.963460	233.854501	48.442394
1616.689751	226.967062	48.447399
1613.411272	232.295236	48.452404
1609.672501	229.937294	48.457409
1606.060349	231.414043	48.462413
1602.811572	233.301716	48.467418
1599.276909	226.313015	48.472423
1595.461185	237.840816	48.477428
1592.196369	237.299363	48.482433
1588.484237	236.731198	48.487437
1584.806618	239.106865	48.492442
1581.798379	221.741659	48.497447
1578.144230	229.565588	48.502452
1575.110724	230.007558	48.507457
1571.190507	231.083415	48.512461
1567.221825	227.016828	48.517466
1564.338372	221.927252	48.522471
1560.162662	237.658721	48.527476
1557.230769	224.289726	48.532481
1553.270878	230.184981	48.537485
1549.978613	229.283840	48.542490
1547.215817	228.848687	48.547495
1543.259882	241.051767	48.552500
1539.831297	224.167546	48.557505
1535.921143	231.544507	48.562509
1532.409867	228.499315	48.567514
1528.868646	227.434557	48.572519
1525.439027	233.409046	48.577524
1522.166523	228.805151	48.582529
1518.459098	227.180626	48.587533
1515.227838	225.492616	48.592538
1511.714375	229.128689	48.597543
1508.199165	227.191673	48.602548
1504.824415	225.829729	48.607553
1500.823250	233.519570	48.612557
1497.713891	229.695375	48.617562
1494.164665	227.477384	48.622567
1490.321423	227.491867	48.627572
1487.129914	227.671776	48.632577
1483.640465	219.423145	48.637581
1479.875434	235.913016	48.642586
1476.576464	216.559797	48.647591
1472.771282	236.763691	48.652596
1469.703467	224.760478	48.657601
1466.178912	220.083870	48.662605
1462.544773	226.089768	48.667610
1459.030692	224.733380	48.672615
1455.178882	223.385673	48.677620
1451.965491	231.347448	48.682625
1448.506614	228.974281	48.687629
1444.928802	225.839291	48.692634
1441.882441	224.835859	48.697639
1438.470591	227.610108	48.702644
1434.839940	216.724454	48.707649
1431.118458	226.978405	48.712653
1427.006024	230.673614	48.717658
1423.967323	224.684726	48.722663
1420.135010	219.703084	48.727668
1416.901667	218.149441	48.732673
1413.795377	222.817482	48.737677
1410.062497	227.672108	48.742682
1406.659657	218.831499	48.747687
1403.089932	229.712730	48.752692
1399.595456	219.494917	48.757697
1395.931986	224.033345	48.762701
1392.161255	217.274629	48.767706
1389.092478	221.938462	48.772711
1385.790640	218.108801	48.777716
1382.070762	213.966933	48.782721
1378.410620	216.378587	48.787725
1374.913256	221.328825	48.792730
1371.466691	221.708338	48.797735
1367.878200	223.533994	48.802740
1364.422327	226.057064	48.807745
1360.897058	224.284173	48.812749
1357.308510	229.979032	48.817754
1354.355353	216.203456	48.822759
1350.556327	225.929802	48.827764
1346.942113	223.062905	48.832769
1343.331685	223.268417	48.837773
1339.637000	223.437820	48.842778
1336.365418	220.559658	48.847783
1332.806073	223.896369	48.852788
1329.480787	221.080645	48.857793
1326.280247	218.508436	48.862797
1322.491373	223.814619	48.867802
1318.802799	216.015973	48.872807
1314.913330	227.906285	48.877812
1311.630230	218.117418	48.882817
1308.540425	213.718086	48.887821
1304.978731	225.876607	48.892826
1301.634303	210.247977	48.897831
1298.111426	223.944153	48.902836
1294.607978	214.024350	48.907841
1290.766291	220.973597	48.912845
1287.062090	230.834280	48.917850
1283.865541	219.979273	48.922855
1279.996018	228.714847	48.927860
1276.910530	222.301052	48.932865
1273.943595	225.690258	48.937869
1270.037388	227.860725	48.942874
1266.814527	220.863962	48.947879
1262.773862	227.915031	48.952884
1259.279755	227.749480	48.957889
1255.938996	226.609747	48.962893
1252.067185	224.668984	48.967898
1248.650784	218.244716	48.972903
1245.281996	221.640184	48.977908
1241.649241	219.245120	48.982913
1238.286011	220.454449	48.987917
1234.886923	218.218819	48.992922
1231.357469	219.392155	48.997927
1227.602940	216.735932	49.002932
1224.375419	227.695212	49.007937
1221.144827	216.915712	49.012941
1217.658671	214.945938	49.017946
1214.316226	217.376263	49.022951
1210.299943	212.048453	49.027956
1206.725309	211.511170	49.032961
1203.154262	225.444411	49.037965
1199.656646	229.377532	49.042970
1196.311437	219.927015	49.047975
1192.969926	221.382182	49.052980
1189.312504	217.897028	49.057985
1185.677257	222.044956	49.062989
1182.116761	223.923206	49.067994
1178.977565	220.897681	49.072999
1175.409980	220.283779	49.078004
1172.001464	223.842603	49.083009
1168.211693	222.483042	49.088013
1164.513608	222.480353	49.093018
1161.481218	209.592261	49.098023
1157.897922	217.221667	49.103028
1154.072431	217.338178	49.108033
1150.795714	211.115745	49.113037
1147.243958	221.078089	49.118042
1143.593790	210.513322	49.123047
1140.285181	220.968367	49.128052
1136.773159	213.356252	49.133057
1133.224796	218.840950	49.138061
1129.343396	214.214267	49.143066
1126.278163	211.776978	49.148071
1122.540631	215.426839	49.153076
1119.214039	208.432884	49.158081
1115.626451	207.277146	49.163085
1112.061586	207.676810	49.168090
1108.745278	211.617725	49.173095
1105.309496	213.375386	49.178100
1102.280641	208.884211	49.183105
1098.563968	208.150334	49.188109
1094.594285	206.615217	49.193114
1091.252241	215.378922	49.198119
1087.367084	218.314046	49.203124
1083.743022	213.238840	49.208129
1081.168435	207.953876	49.213133
1077.285578	216.019797	49.218138
1073.802202	201.143331	49.223143
1070.473658	212.881742	49.228148
1066.782345	209.227143	49.233153
1063.234745	203.843560	49.238157
1059.444885	215.367204	49.243162
1056.305229	206.580633	49.248167
1052.333974	212.150574	49.253172
1049.442651	205.755360	49.258177
1045.966270	207.401169	49.263181
1042.071487	222.958906	49.268186
1038.534226	213.832805	49.273191
1035.016915	226.201737	49.278196
1031.521700	208.573769	49.283201
1028.448363	207.861179	49.288205
1024.674077	213.711847	49.293210
1021.249283	204.814426	49.298215
1017.451829	210.386175	49.303220
1014.099928	210.070401	49.308225
1010.701816	208.565371	49.313229
1006.859804	212.376874	49.318234
1003.481017	202.378470	49.323239
1000.033327	209.260534	49.328244
997.065402	206.964499	49.333249
993.500172	212.076463	49.338253
989.635460	215.880476	49.343258
986.147714	203.807293	49.348263
982.507012	210.838831	49.353268
979.086422	203.236482	49.358273
975.678412	204.884749	49.363277
971.896590	208.902189	49.368282
968.325705	208.481123	49.373287
964.889250	210.866807	49.378292
961.576297	205.360387	49.383297
958.425900	210.894587	49.388301
954.575293	209.513526	49.393306
951.365403	208.863770	49.398311
947.547394	205.173531	49.403316
944.235092	211.307953	49.408321
940.458271	212.139495	49.413325
937.159272	214.469151	49.418330
934.173576	209.839031	49.423335
929.978439	216.307265	49.428340
926.410543	215.208952	49.433345
922.872137	207.944152	49.438349
919.495977	218.571339	49.443354
915.997815	203.246365	49.448359
912.451378	204.849843	49.453364
908.740120	208.840570	49.458369
905.455162	201.075583	49.463373
901.606874	211.907698	49.468378
898.629893	197.071946	49.473383
894.805932	204.367002	49.478388
891.724874	195.889214	49.483393
888.234537	201.435471	49.488397
884.490595	203.503093	49.493402
881.477453	209.676341	49.498407
877.426778	205.675324	49.503412
874.114066	208.233193	49.508417
870.300571	210.273438	49.513421
867.151560	203.557321	49.518426
863.914960	205.622472	49.523431
859.671935	214.325006	49.528436
856.173595	208.218848	49.533441
853.200897	205.246005	49.538445
849.325565	214.120458	49.543450
846.171752	209.626169	49.548455
842.380746	215.047875	49.553460
839.025128	211.174405	49.558465
835.864819	214.392979	49.563469
831.874267	211.949990	49.568474
828.462413	211.835996	49.573479
825.004904	197.962601	49.578484
821.343911	210.968571	49.583489
818.074707	209.907810	49.588493
814.135361	214.160889	49.593498
811.020607	200.262373	49.598503
807.429330	213.744491	49.603508
804.031346	213.083937	49.608513
800.529986	201.667111	49.613517
796.997931	210.848544	49.618522
793.345926	211.438273	49.623527
790.075965	212.150682	49.628532
786.452580	211.983541	49.633537
783.325992	203.273201	49.638541
779.264203	212.467241	49.643546
775.950881	205.258098	49.648551
772.444464	212.145917	49.653556
769.087460	219.779366	49.658561
765.623872	210.788466	49.663565
761.863666	207.409227	49.668570
758.658279	195.938228	49.673575
755.049578	205.008619	49.678580
751.016730	212.278065	49.683585
747.651226	209.972331	49.688589
743.951942	208.941394	49.693594
740.812490	201.927210	49.698599
737.434333	207.692575	49.703604
733.942037	209.276746	49.708609
730.470012	205.614742	49.713613
727.022430	211.250500	49.718618
723.687576	193.378456	49.723623
719.934590	207.710092	49.728628
716.116297	195.756595	49.733633
712.855330	205.085867	49.738637
709.169140	207.637618	49.743642
705.793603	206.663237	49.748647
702.704045	207.261151	49.753652
698.853559	203.732304	49.758657
695.410055	195.784475	49.763661
691.418933	204.658589	49.768666
688.373078	198.320452	49.773671
684.749017	200.113952	49.778676
681.228106	207.167576	49.783681
677.624802	209.347143	49.788685
674.147634	200.246970	49.793690
671.533064	198.002731	49.798695
667.590479	199.146027	49.803700
664.010709	203.160051	49.808705
660.766032	201.949409	49.813709
656.403368	207.447861	49.818714
653.155225	202.877703	49.823719
649.792662	207.468608	49.828724
646.056374	204.348406	49.833729
642.879819	206.318308	49.838733
639.199912	198.213429	49.843738
635.960835	203.334243	49.848743
631.961406	198.612339	49.853748
628.979849	203.267789	49.858753
625.608132	201.738181	49.863757
621.502335	202.772119	49.868762
618.104783	194.085123	49.873767
614.263096	201.382850	49.878772
611.505601	198.411971	49.883777
608.110985	195.838342	49.888781
604.312513	204.238509	49.893786
601.260851	202.264590	49.898791
596.780132	195.607668	49.903796
593.456984	195.533504	49.908801
590.308693	199.112163	49.913805
586.489697	195.409685	49.918810
583.061517	194.870056	49.923815
579.735298	200.326408	49.928820
576.408677	207.771319	49.933825
573.061019	198.271971	49.938829
569.140810	205.445660	49.943834
565.902637	196.252118	49.948839
562.461440	205.143495	49.953844
558.780739	200.657166	49.958849
555.291566	197.303432	49.963853
551.526977	213.994319	49.968858
548.136590	203.898371	49.973863
544.638289	198.021670	49.978868
541.264654	210.690346	49.983873
538.093799	200.019489	49.988877
534.188690	202.661555	49.993882
530.368964	197.283085	49.998887
527.335939	190.039536	50.003892
523.362271	195.919634	50.008897
520.445390	199.023160	50.013901
516.739204	200.188761	50.018906
513.340724	190.719356	50.023911
509.487486	199.617843	50.028916
505.716860	195.693936	50.033921
502.696203	193.928237	50.038925
498.681793	205.803824	50.043930
495.411186	189.714878	50.048935
492.018542	206.020361	50.053940
488.584304	205.778240	50.058945
485.427205	191.113377	50.063949
481.813617	193.846520	50.068954
478.074634	193.701703	50.073959
474.453120	190.883672	50.078964
471.078427	198.079667	50.083969
467.509051	195.822955	50.088973
463.870652	204.979971	50.093978
460.791757	195.754953	50.098983
457.168587	204.167671	50.103988
453.582149	200.951801	50.108993
450.536238	190.908527	50.113997
446.702913	202.516763	50.119002
442.864839	186.832159	50.124007
439.488913	201.633764	50.129012
436.110600	196.115551	50.134017
432.662065	194.377060	50.139021
429.350421	197.490290	50.144026
425.826641	194.592509	50.149031
422.145887	190.733721	50.154036
418.330489	204.168363	50.159041
415.302950	200.398289	50.164045
411.349353	198.018720	50.169050
408.019849	199.329826	50.174055
404.462001	201.605022	50.179060
400.782878	195.802970	50.184065
397.821616	192.211574	50.189069
394.123143	198.799215	50.194074
390.988757	193.510358	50.199079
386.912145	204.381808	50.204084
383.326945	193.328252	50.209089
380.037354	195.376733	50.214093
376.347930	202.927733	50.219098
373.005708	195.056600	50.224103
369.587131	200.292815	50.229108
366.071235	193.703095	50.234113
362.632181	197.177172	50.239117
358.978699	199.366971	50.244122
355.619484	190.682586	50.249127
351.662475	191.860021	50.254132
348.590106	190.515218	50.259137
345.163442	194.642520	50.264141
341.503725	187.300066	50.269146
338.438643	191.044543	50.274151
334.338785	201.217536	50.279156
330.954217	196.924723	50.284161
327.463395	192.454130	50.289165
323.842429	191.185270	50.294170
320.748442	195.483839	50.299175
316.946449	189.913756	50.304180
313.527258	199.363636	50.309185
310.117430	189.446863	50.314189
306.682894	194.650819	50.319194
303.034298	193.315110	50.324199
299.458325	185.498626	50.329204
295.722601	189.755046	50.334209
292.269809	182.546450	50.339213
288.832839	191.175706	50.344218
285.397381	175.203732	50.349223
281.996207	189.364453	50.354228
278.465788	182.835397	50.359233
275.227994	182.761403	50.364237
271.348767	191.196774	50.369242
267.759429	177.574731	50.374247
264.417888	184.835676	50.379252
260.609785	190.731577	50.384257
257.569405	189.165777	50.389261
253.660801	194.050701	50.394266
250.323227	194.594602	50.399271
247.253488	193.127674	50.404276
243.405677	190.773947	50.409281
240.347159	186.258127	50.414285
236.363044	188.502026	50.419290
232.738339	191.163640	50.424295
228.963935	180.035602	50.429300
225.613129	189.832530	50.434305
222.472856	189.312611	50.439309
218.726444	185.729092	50.444314
215.706580	191.491823	50.449319
212.305851	182.256697	50.454324
208.820375	193.346159	50.459329
204.939805	187.522272	50.464333
201.076304	184.934888	50.469338
197.769025	187.854933	50.474343
194.365009	180.620582	50.479348
190.615684	186.063750	50.484353
187.723623	173.513372	50.489357
183.837564	189.852329	50.494362
180.311856	183.729209	50.499367
176.910538	180.933574	50.504372
173.269617	183.989063	50.509377
169.701362	185.541683	50.514381
166.299963	195.508199	50.519386
162.872075	183.474819	50.524391
159.561381	188.205952	50.529396
155.930468	199.375113	50.534401
152.271298	187.880326	50.539405
148.459299	190.332413	50.544410
145.211810	183.708054	50.549415
142.220626	190.532135	50.554420
138.133653	196.267797	50.559425
134.648537	174.061582	50.564429
131.414663	190.718393	50.569434
128.047438	183.648377	50.574439
124.526458	191.461511	50.579444
120.910319	181.850155	50.584449
117.294426	190.217922	50.589453
113.488150	198.295443	50.594458
110.194114	184.035152	50.599463
106.940618	198.172631	50.604468
103.283254	191.612469	50.609473
99.890796	181.555934	50.614477
96.044767	183.121247	50.619482
92.894578	181.719090	50.624487
88.872990	182.928565	50.629492
85.634176	180.233098	50.634497
82.655655	182.404053	50.639501
78.684483	188.669426	50.644506
75.463957	184.943555	50.649511
71.746488	190.841352	50.654516
68.264870	185.386995	50.659521
64.605844	188.039375	50.664525
60.953059	202.302836	50.669530
57.931276	186.090207	50.674535
54.123457	182.201739	50.679540
50.701388	185.878562	50.684545
47.309495	181.030224	50.689549
43.485472	188.303914	50.694554
40.332455	190.420459	50.699559
36.906538	191.072693	50.704564
33.147330	188.105231	50.709569
29.892041	179.525621	50.714573
26.100398	184.372698	50.719578
23.013797	181.624389	50.724583
19.374947	186.994146	50.729588
15.667584	182.151887	50.734593
11.950976	179.610592	50.739597
8.478713	187.093129	50.744602
4.919604	182.086781	50.749607
1.969828	188.397880	50.754612