Thu Jun 16 10:42:53 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.319194	102.398599	0.000000
1.158378	111.405845	0.005005
0.696778	105.857545	0.010010
0.832899	99.272074	0.015014
0.590345	101.320643	0.020019
0.796576	91.647850	0.025024
0.680704	77.013514	0.030029
0.390861	78.274448	0.035034
0.124610	65.858248	0.040038
-0.311608	56.556531	0.045043
-0.534368	48.444232	0.050048
-0.597318	37.099086	0.055053
-0.904681	38.044852	0.060058
-1.406218	34.009621	0.065062
-2.347649	17.686184	0.070067
-2.308294	16.195326	0.075072
-2.511103	18.794709	0.080077
-2.435881	15.409892	0.085082
-2.308034	9.203078	0.090086
-3.437617	5.968234	0.095091
-3.809023	3.538598	0.100096
-3.770124	10.253616	0.105101
-3.944077	7.830613	0.110106
-3.903130	2.169017	0.115110
-4.713726	13.893758	0.120115
-5.181346	-1.857238	0.125120
-5.529386	3.968532	0.130125
-5.429356	-1.828709	0.135130
-5.418372	-2.549326	0.140134
-5.520054	-0.779167	0.145139
-6.071915	11.333240	0.150144
-6.791021	-2.018673	0.155149
-6.920448	-0.903921	0.160154
-6.852463	-5.320242	0.165158
-7.245371	4.212643	0.170163
-6.995844	1.040233	0.175168
-6.883069	10.310301	0.180173
-7.900135	10.133373	0.185178
-8.123975	-2.402046	0.190182
-8.224145	-0.841677	0.195187
-8.366551	-2.126005	0.200192
-8.607603	5.341929	0.205197
-9.686042	7.189154	0.210202
-10.069266	-4.657662	0.215206
-10.132961	-3.997122	0.220211
-9.727872	9.603667	0.225216
-9.894502	7.927938	0.230221
-10.316584	4.590778	0.235226
-10.168433	-6.963935	0.240230
-10.718097	-0.237980	0.245235
-11.217289	2.612421	0.250240
-11.658858	-1.095216	0.255245
-11.979636	4.217391	0.260250
-11.456108	-0.465402	0.265254
-11.705990	3.918407	0.270259
-12.068790	6.384409	0.275264
-12.751113	-4.297899	0.280269
-13.095308	0.202121	0.285274
-13.158209	-2.736642	0.290278
-13.506387	7.799162	0.295283
-13.568505	-3.840077	0.300288
-13.578531	-3.746290	0.305293
-13.982331	7.441531	0.310298
-14.424075	-6.062758	0.315302
-14.677454	10.661794	0.320307
-14.524837	-0.790075	0.325312
-14.797710	1.660473	0.330317
-15.530509	-3.837837	0.335322
-15.778245	-10.690019	0.340326
-15.932198	5.050800	0.345331
-16.207548	-4.091599	0.350336
-16.370021	-4.220931	0.355341
-16.156295	-4.813359	0.360346
-16.793907	-5.027244	0.365350
-17.723862	-0.395006	0.370355
-17.647071	-3.608815	0.375360
-17.908642	-5.164477	0.380365
-18.217846	8.372731	0.385370
-17.908982	-0.307147	0.390374
-17.982296	-4.412837	0.395379
-17.941883	-2.235145	0.400384
-18.608245	-1.249783	0.405389
-19.472060	2.158089	0.410394
-19.466754	-4.828943	0.415398
-19.283236	-9.864364	0.420403
-19.667158	-1.112329	0.425408
-20.129468	-1.182047	0.430413
-20.645555	8.602144	0.435418
-20.661229	-0.812539	0.440422
-21.000034	8.654879	0.445427
-21.064189	7.141568	0.450432
-21.348984	1.929404	0.455437
-22.246828	5.275027	0.460442
-22.386070	2.892361	0.465446
-22.193782	11.585187	0.470451
-22.528460	8.409384	0.475456
-22.675566	10.428455	0.480461
-22.857179	9.729209	0.485466
-22.819548	1.090701	0.490470
-22.858069	12.222501	0.495475
-23.791574	8.694024	0.500480
-24.237221	2.421676	0.505485
-24.412846	6.402941	0.510490
-24.180504	3.170231	0.515494
-24.140243	7.973710	0.520499
-24.418831	0.880384	0.525504
-25.292515	4.097218	0.530509
-26.031422	6.482821	0.535514
-26.158225	-5.788354	0.540518
-25.860023	9.020841	0.545523
-25.721613	5.490232	0.550528
-26.040167	3.156733	0.555533
-26.589070	9.767833	0.560538
-27.020893	2.865764	0.565542
-27.369580	9.258407	0.570547
-27.506169	6.540373	0.575552
-27.608586	5.446152	0.580557
-27.654789	3.597511	0.585562
-27.770092	3.002239	0.590566
-28.878170	3.575323	0.595571
-29.275946	-5.661477	0.600576
-29.176636	1.443592	0.605581
-29.609855	6.100190	0.610586
-29.346910	2.533710	0.615590
-29.675918	7.735411	0.620595
-29.588198	5.541153	0.625600
-29.737422	11.416347	0.630605
-30.339708	14.832302	0.635610
-30.641439	2.370822	0.640614
-30.828657	12.415173	0.645619
-31.062986	0.632045	0.650624
-31.195691	8.020711	0.655629
-31.897502	16.112913	0.660634
-32.041473	7.158831	0.665638
-32.815636	7.210201	0.670643
-32.930133	9.076396	0.675648
-32.832155	7.963954	0.680653
-33.032312	12.516138	0.685658
-32.902155	-2.979670	0.690662
-33.095914	0.352590	0.695667
-32.993414	-5.693169	0.700672
-33.807397	1.301398	0.705677
-34.577009	13.495961	0.710682
-34.641907	7.200842	0.715686
-34.543151	6.186629	0.720691
-34.466559	-1.854063	0.725696
-35.178828	-4.434634	0.730701
-35.877027	-1.311222	0.735706
-35.986834	-6.867793	0.740710
-36.327602	2.581398	0.745715
-36.314725	1.229777	0.750720
-35.839118	-8.178190	0.755725
-36.113648	-3.644401	0.760730
-36.741498	-0.309756	0.765734
-36.952803	-5.558330	0.770739
-37.525098	-4.858625	0.775744
-37.368239	-1.023563	0.780749
-38.078571	1.312530	0.785754
-38.646711	6.593902	0.790758
-38.884885	8.486554	0.795763
-38.999750	-3.952332	0.800768
-39.242987	-6.536820	0.805773
-38.971019	8.337084	0.810778
-38.898740	-10.117436	0.815782
-39.171648	-1.799671	0.820787
-39.665113	5.290402	0.825792
-39.868581	-7.669426	0.830797
-40.485636	7.466131	0.835802
-40.236333	-13.024844	0.840806
-40.967174	-1.337661	0.845811
-41.722825	0.942289	0.850816
-41.884717	-1.787838	0.855821
-42.596117	-0.362929	0.860826
-42.090668	2.219438	0.865830
-42.118804	10.411028	0.870835
-42.328746	9.182946	0.875840
-41.833520	4.236096	0.880845
-42.481907	12.501680	0.885850
-42.946651	5.983389	0.890854
-43.779528	9.543208	0.895859
-43.825962	2.616223	0.900864
-43.557591	5.981814	0.905869
-44.250773	8.590120	0.910874
-44.954850	3.091209	0.915878
-45.452008	14.362534	0.920883
-45.139658	5.444224	0.925888
-45.112349	3.168006	0.930893
-45.163714	12.344051	0.935898
-45.306942	0.842520	0.940902
-45.739224	12.295101	0.945907
-45.946200	8.817822	0.950912
-46.069839	8.881748	0.955917
-47.008137	11.373014	0.960922
-46.901436	1.987335	0.965926
-46.935623	8.797297	0.970931
-47.659748	6.193725	0.975936
-48.055299	9.321285	0.980941
-48.437013	7.791200	0.985946
-48.484107	4.422458	0.990950
-48.950673	10.921890	0.995955
-48.589363	5.505284	1.000960
-48.584786	8.575103	1.005965
-49.059784	7.067835	1.010970
-48.851894	-2.809086	1.015974
-49.276461	5.279713	1.020979
-49.706609	9.996378	1.025984
-49.898706	0.289144	1.030989
-50.834461	2.156104	1.035994
-51.307064	1.826066	1.040998
-51.567836	6.972195	1.046003
-51.592214	5.955444	1.051008
-51.473130	0.823037	1.056013
-51.846341	4.005702	1.061018
-51.577559	-7.657928	1.066022
-51.802685	2.948197	1.071027
-52.172919	-3.174027	1.076032
-52.798484	6.699187	1.081037
-53.784208	-1.062454	1.086042
-53.328048	2.615711	1.091046
-53.314007	4.134613	1.096051
-53.189548	-4.667796	1.101056
-53.285858	-9.556345	1.106061
-54.570236	5.181428	1.111066
-54.659645	5.824121	1.116070
-54.949449	3.812118	1.121075
-55.047565	3.581687	1.126080
-54.812220	-2.507040	1.131085
-55.102043	3.503652	1.136090
-55.765059	-7.551390	1.141094
-56.286596	2.661064	1.146099
-56.560542	6.039724	1.151104
-56.593852	-4.782289	1.156109
-57.096880	5.843918	1.161114
-56.840858	-1.204968	1.166118
-56.654581	6.625332	1.171123
-57.138326	1.462132	1.176128
-57.371888	4.399156	1.181133
-58.253497	4.853923	1.186138
-57.936830	-3.286719	1.191142
-58.574516	-3.149579	1.196147
-59.722737	1.325079	1.201152
-58.829066	-2.524890	1.206157
-59.326816	10.024287	1.211162
-59.604848	1.698297	1.216166
-59.927272	2.448654	1.221171
-59.903819	6.969208	1.226176
-59.975015	-1.436738	1.231181
-60.311383	7.652925	1.236186
-60.878961	-3.150541	1.241190
-61.536994	-1.899596	1.246195
-61.425401	-2.724937	1.251200
-61.280083	2.257101	1.256205
-61.833172	-1.721648	1.261210
-61.776769	-3.007557	1.266214
-61.722768	7.658494	1.271219
-62.679879	7.134765	1.276224
-63.032529	4.138230	1.281229
-63.240506	5.727366	1.286234
-63.145472	2.814987	1.291238
-63.142467	0.912144	1.296243
-63.374467	0.536819	1.301248
-63.963271	1.768925	1.306253
-64.611960	7.103268	1.311258
-64.396315	2.711674	1.316262
-65.108353	5.565193	1.321267
-64.935157	0.911685	1.326272
-64.748793	-5.790462	1.331277
-65.467517	4.000085	1.336282
-65.672040	5.475495	1.341286
-66.042519	6.803518	1.346291
-66.354892	6.409709	1.351296
-66.053185	-1.146406	1.356301
-66.697121	8.507085	1.361306
-67.148742	-7.562817	1.366310
-67.101236	9.745356	1.371315
-67.306209	11.905101	1.376320
-67.660248	6.871404	1.381325
-68.188554	10.449554	1.386330
-68.598948	7.048316	1.391334
-69.163986	3.628045	1.396339
-68.895128	3.637661	1.401344
-68.798059	6.588903	1.406349
-69.800908	6.374417	1.411354
-69.278623	4.104494	1.416358
-69.747288	6.197326	1.421363
-70.067462	-3.465750	1.426368
-69.713711	0.584785	1.431373
-70.756449	3.913517	1.436378
-70.905450	8.867051	1.441382
-70.950913	-2.396401	1.446387
-71.108272	-2.042780	1.451392
-71.023282	0.665994	1.456397
-71.719456	5.101067	1.461402
-72.096379	0.228409	1.466406
-72.497164	0.184042	1.471411
-72.610444	3.444106	1.476416
-72.862957	-1.315733	1.481421
-73.131311	5.139396	1.486426
-73.140969	2.922265	1.491430
-73.467011	11.750074	1.496435
-74.281794	3.146985	1.501440
-74.535843	-0.879408	1.506445
-74.603300	6.797885	1.511450
-74.529298	0.898106	1.516454
-74.781747	1.799875	1.521459
-75.065211	3.980779	1.526464
-74.893448	-3.951432	1.531469
-75.065076	-2.749993	1.536474
-75.719980	-6.156001	1.541478
-76.083001	3.724429	1.546483
-76.465369	7.117063	1.551488
-76.544233	2.349636	1.556493
-76.718160	6.716848	1.561498
-76.326060	-3.563720	1.566502
-77.229168	-4.269409	1.571507
-77.968381	1.161875	1.576512
-77.928843	-9.103534	1.581517
-78.074939	11.596865	1.586522
-77.933915	0.046783	1.591526
-78.547912	1.487661	1.596531
-79.404493	8.302819	1.601536
-79.076479	4.967088	1.606541
-79.848370	8.456949	1.611546
-79.870964	-1.010646	1.616550
-80.084506	15.434147	1.621555
-79.930471	0.791201	1.626560
-79.663272	5.846817	1.631565
-79.801339	13.424205	1.636570
-80.489887	6.678910	1.641574
-81.278716	-2.198281	1.646579
-81.525669	7.972446	1.651584
-81.281977	8.363669	1.656589
-81.763476	4.379699	1.661594
-82.420177	-0.420182	1.666598
-82.529644	-5.484428	1.671603
-82.621795	-0.664695	1.676608
-82.839108	-5.032382	1.681613
-83.167424	1.835063	1.686618
-82.837702	9.645404	1.691622
-83.094670	-1.127116	1.696627
-83.925191	-0.198079	1.701632
-84.058408	5.790382	1.706637
-84.801962	-0.376292	1.711642
-84.991754	0.870077	1.716646
-84.754212	5.456761	1.721651
-85.084715	8.611455	1.726656
-84.732902	-1.071523	1.731661
-85.066488	5.154463	1.736666
-85.662526	-0.118523	1.741670
-85.950917	3.162885	1.746675
-86.196761	3.672698	1.751680
-87.033309	-5.422026	1.756685
-87.419472	10.469728	1.761690
-87.026960	-3.028785	1.766694
-87.372828	1.036945	1.771699
-87.813521	5.895933	1.776704
-87.917668	3.003351	1.781709
-88.031975	3.679360	1.786714
-87.833659	-0.391804	1.791718
-88.160758	-1.746921	1.796723
-89.237583	9.289118	1.801728
-89.332300	0.422699	1.806733
-89.786054	-0.173560	1.811738
-89.664534	-0.725496	1.816742
-89.928283	-0.568863	1.821747
-89.826453	-0.375376	1.826752
-89.572763	-3.644661	1.831757
-90.473286	3.028397	1.836762
-90.761121	0.685485	1.841766
-90.989424	0.838628	1.846771
-91.147786	4.020215	1.851776
-91.227005	-0.518374	1.856781
-92.281706	-0.599096	1.861786
-92.068790	4.206327	1.866790
-92.436764	2.465818	1.871795
-92.785500	11.532567	1.876800
-92.431328	-4.944367	1.881805
-92.391542	10.621775	1.886810
-93.299955	-2.053932	1.891814
-94.236164	3.102409	1.896819
-94.132771	12.111897	1.901824
-94.178781	-10.137596	1.906829
-94.489750	5.318601	1.911834
-94.336788	6.666761	1.916838
-94.343025	2.146100	1.921843
-94.907352	6.729167	1.926848
-95.504220	0.848615	1.931853
-95.698548	7.707927	1.936858
-95.836073	1.379635	1.941862
-95.742947	8.362800	1.946867
-96.472796	-0.271288	1.951872
-96.659569	3.133907	1.956877
-97.292897	12.230821	1.961882
-97.580409	0.147018	1.966886
-97.555471	-1.746229	1.971891
-97.556240	8.461746	1.976896
-97.575509	-1.883722	1.981901
-97.684007	16.209964	1.986906
-98.141158	9.927489	1.991910
-98.499195	-0.776730	1.996915
-99.225421	6.155922	2.006912
-98.483712	4.581894	2.016909
-98.075557	6.256836	2.026906
-97.752237	3.656290	2.036902
-96.535857	6.825891	2.046899
-96.262624	2.027133	2.056896
-96.323475	3.191650	2.066893
-95.822357	3.240082	2.076890
-95.029361	0.151534	2.086886
-94.755275	-0.814664	2.096883
-93.534802	2.266000	2.106880
-93.012390	3.348445	2.116877
-93.240716	1.264219	2.126874
-92.923894	3.719847	2.136870
-92.296859	-0.090270	2.146867
-91.752278	5.813603	2.156864
-90.701270	-4.431995	2.166861
-90.410453	0.307716	2.176858
-90.446119	-1.164209	2.186854
-89.494648	-3.007802	2.196851
-88.714929	-1.297464	2.206848
-88.943675	4.285756	2.216845
-88.060989	1.375351	2.226842
-87.382050	6.645079	2.236838
-87.174144	5.151173	2.246835
-86.355324	-2.437057	2.256832
-85.653619	-0.926597	2.266829
-85.863270	-3.796788	2.276826
-85.120382	-4.828808	2.286822
-84.615762	-0.114455	2.296819
-83.976804	4.300720	2.306816
-83.108502	-1.101692	2.316813
-82.743964	4.621388	2.326810
-82.667393	6.568299	2.336806
-82.468780	2.840050	2.346803
-81.519297	-0.405984	2.356800
-80.983291	-1.621473	2.366797
-80.002308	-0.089751	2.376794
-79.737522	3.148960	2.386790
-79.375497	2.129754	2.396787
-79.019420	-2.038947	2.406784
-78.832079	4.915566	2.416781
-78.105688	8.761102	2.426778
-77.916074	2.831503	2.436774
-76.731640	3.086065	2.446771
-76.364764	6.728163	2.456768
-76.173141	2.399748	2.466765
-75.066748	6.167121	2.476762
-74.845079	6.087342	2.486758
-74.334641	-1.328126	2.496755
-74.444854	8.518889	2.506752
-73.461734	4.788857	2.516749
-72.951646	1.430180	2.526746
-72.658607	5.410307	2.536742
-71.424569	0.821158	2.546739
-71.256255	0.448722	2.556736
-71.367860	1.517711	2.566733
-70.654848	-0.725002	2.576730
-69.743501	4.456090	2.586726
-69.573428	1.741296	2.596723
-68.974835	5.141367	2.606720
-68.113352	5.544280	2.616717
-68.174653	7.376673	2.626714
-67.613649	6.119812	2.636710
-66.999010	3.785439	2.646707
-66.585984	-5.647654	2.656704
-65.736228	3.098203	2.666701
-65.125773	8.713870	2.676698
-65.223902	9.686347	2.686694
-64.824633	9.419714	2.696691
-63.955073	-0.942487	2.706688
-63.571747	-1.376139	2.716685
-62.624012	2.827935	2.726682
-62.244235	4.414470	2.736678
-62.013300	2.646299	2.746675
-61.711469	1.815735	2.756672
-60.846049	1.110924	2.766669
-60.485131	-0.891844	2.776666
-60.198118	3.286096	2.786662
-59.071897	-4.265068	2.796659
-58.797798	0.597475	2.806656
-58.939401	1.490112	2.816653
-57.848294	2.018657	2.826650
-57.377906	-2.420676	2.836646
-57.000599	4.527189	2.846643
-55.867341	0.750468	2.856640
-55.615926	6.859560	2.866637
-55.408814	5.505953	2.876634
-55.611494	5.301363	2.886630
-54.710536	13.060353	2.896627
-53.758889	-0.113647	2.906624
-53.066162	13.283333	2.916621
-52.607916	7.412857	2.926618
-52.299354	0.730309	2.936614
-52.468734	4.967378	2.946611
-51.540959	7.493523	2.956608
-50.815799	6.976510	2.966605
-50.676311	5.172680	2.976602
-49.375377	9.430009	2.986598
-49.299140	10.304574	2.996595
-49.390072	8.520795	3.006592
-48.538629	-0.525134	3.016589
-47.878636	1.195612	3.026586
-47.439685	4.093054	3.036582
-46.600483	1.763305	3.046579
-45.960708	-0.606187	3.056576
-45.823679	4.042780	3.066573
-45.939196	-2.752376	3.076570
-44.714272	4.039014	3.086566
-44.469502	3.593243	3.096563
-44.242591	-1.806738	3.106560
-43.274928	1.336709	3.116557
-42.660759	-1.113008	3.126554
-42.588311	-4.899034	3.136550
-41.945422	3.722771	3.146547
-41.440737	-0.911442	3.156544
-40.959865	2.043229	3.166541
-40.023152	2.646584	3.176538
-39.913878	-4.429213	3.186534
-39.536308	-2.303223	3.196531
-38.773054	5.810474	3.206528
-38.340395	6.751388	3.216525
-37.923091	7.107249	3.226522
-37.643814	0.814238	3.236518
-36.671257	-1.477983	3.246515
-36.609135	-5.782131	3.256512
-35.642634	-0.171468	3.266509
-35.152602	-7.389064	3.276506
-35.247124	-2.143974	3.286502
-34.440271	-7.075220	3.296499
-33.276069	-9.326656	3.306496
-33.292846	-3.258639	3.316493
-33.346869	-2.069271	3.326490
-32.564293	-3.500345	3.336486
-31.781623	2.296425	3.346483
-31.345531	6.066665	3.356480
-30.528604	5.429585	3.366477
-30.122097	-1.518223	3.376474
-29.935001	0.447565	3.386470
-29.566453	-6.133916	3.396467
-28.599387	-8.042802	3.406464
-28.463420	-0.642794	3.416461
-28.321542	1.801498	3.426458
-26.878417	-3.413097	3.436454
-26.897243	1.595403	3.446451
-26.787892	-4.144066	3.456448
-25.619865	-1.707159	3.466445
-25.078891	-0.900111	3.476442
-24.806724	2.490246	3.486438
-24.339148	-2.514679	3.496435
-23.544957	0.130894	3.506432
-23.156288	-3.298493	3.516429
-22.937634	5.614396	3.526426
-22.842281	3.157369	3.536422
-22.240265	3.220692	3.546419
-21.179548	-4.122430	3.556416
-20.415765	-5.650165	3.566413
-20.112662	-0.613423	3.576410
-19.961535	-0.805856	3.586406
-19.749383	-0.285356	3.596403
-19.125794	4.891836	3.606400
-17.926946	3.134995	3.616397
-17.865368	-0.816866	3.626394
-17.052418	5.310657	3.636390
-16.916611	0.958720	3.646387
-16.378923	2.943915	3.656384
-15.773448	4.525209	3.666381
-15.521863	8.704960	3.676378
-14.919269	3.449589	3.686374
-14.172843	4.568267	3.696371
-13.780604	7.288516	3.706368
-13.482219	5.242543	3.716365
-12.399690	8.801004	3.726362
-12.270994	4.340743	3.736358
-12.206612	2.548781	3.746355
-11.130364	7.629982	3.756352
-10.455219	2.301922	3.766349
-10.415172	1.198575	3.776346
-10.148832	1.286306	3.786342
-9.392136	8.488122	3.796339
-8.859819	4.397618	3.806336
-8.307780	-1.072836	3.816333
-7.519579	8.999006	3.826330
-7.083021	9.114862	3.836326
-7.227705	5.325154	3.846323
-6.445668	4.731330	3.856320
-6.047153	16.861840	3.866317
-5.424335	15.597139	3.876314
-4.444285	16.797773	3.886310
-4.320121	11.368635	3.896307
-4.173344	20.671098	3.906304
-3.520330	22.017148	3.916301
-2.995612	40.036034	3.926298
-2.182709	42.498943	3.936294
-2.132523	45.089822	3.946291
-1.525040	58.114168	3.956288
-1.360892	71.521465	3.966285
-0.915598	85.164232	3.976282
-0.201823	103.983533	3.986278
0.000000	111.907193	3.991283
0.140200	133.038932	3.996288
0.442724	145.527497	4.001293
0.534287	136.412575	4.006298
0.772022	141.367946	4.011302
1.046692	139.133502	4.016307
0.837822	143.876778	4.021312
0.858391	145.265675	4.026317
0.987413	138.719835	4.031322
0.793523	148.430449	4.036326
1.251488	140.638701	4.041331
0.893642	150.431065	4.046336
1.011295	138.723927	4.051341
0.752008	155.893855	4.056346
0.982543	157.208002	4.061350
1.487197	151.913172	4.066355
0.991315	147.939423	4.071360
0.936987	135.361277	4.076365
1.366767	149.966655	4.081370
1.060200	152.422499	4.086374
1.193522	144.159063	4.091379
0.769499	143.563304	4.096384
1.124490	149.635306	4.101389
1.477038	157.011532	4.106394
1.153009	163.216962	4.111398
1.123947	154.413290	4.116403
1.046912	169.685193	4.121408
1.403443	161.590654	4.126413
1.714401	161.623209	4.131418
1.259721	156.145074	4.136422
1.390475	137.222655	4.141427
1.004918	146.144531	4.146432
0.877624	126.590367	4.151437
1.408942	149.016653	4.156442
1.239613	157.651729	4.161446
1.450317	156.231787	4.166451
1.071938	142.444409	4.171456
1.294047	158.764396	4.176461
1.715627	160.850118	4.181466
1.092624	155.034186	4.186470
1.434524	164.152637	4.191475
1.340242	163.499623	4.196480
1.467218	168.210097	4.201485
1.698328	167.853929	4.206490
1.415169	148.434014	4.211494
1.429829	144.063557	4.216499
1.088245	149.043438	4.221504
1.330491	154.521234	4.226509
1.519753	158.566346	4.231514
1.545583	170.532802	4.236518
1.895369	164.344396	4.241523
1.541136	159.865112	4.246528
1.198916	144.540935	4.251533
1.448609	155.525473	4.256538
1.403560	171.905408	4.261542
1.556278	170.873684	4.266547
1.297245	183.179439	4.271552
1.428225	176.226309	4.276557
1.791324	166.177914	4.281562
1.174417	182.468076	4.286566
1.488995	176.054928	4.291571
1.193146	179.221192	4.296576
1.385935	180.319901	4.301581
1.590871	174.207025	4.306586
1.293451	173.197402	4.311590
1.553181	169.934186	4.316595
1.910641	194.014405	4.321600
1.677627	190.723106	4.326605
1.860624	181.393468	4.331610
1.520555	184.557669	4.336614
1.685351	181.696273	4.341619
1.990737	195.929015	4.346624
1.683111	193.591014	4.351629
1.769458	185.982690	4.356634
1.496317	195.838825	4.361638
2.124769	199.821729	4.366643
2.076754	190.151230	4.371648
1.613752	178.891525	4.376653
1.792837	187.801703	4.381658
2.053445	188.166265	4.386662
1.882523	182.903057	4.391667
1.598790	184.980936	4.396672
1.893420	186.406529	4.401677
2.224128	196.172444	4.406682
1.919903	181.805709	4.411686
1.873210	177.007749	4.416691
2.062008	185.594116	4.421696
2.114385	181.323962	4.426701
1.862227	180.173675	4.431706
1.820678	178.776575	4.436710
1.976667	184.302375	4.441715
2.038387	188.583541	4.446720
2.207982	192.684495	4.451725
2.103057	180.013454	4.456730
1.756939	179.547670	4.461734
2.134838	190.411307	4.466739
2.337045	189.714426	4.471744
1.849950	181.537811	4.476749
1.824529	184.327315	4.481754
2.329451	197.019838	4.486758
2.255976	197.782730	4.491763
2.088949	193.653701	4.496768
2.166089	201.915604	4.501773
2.217377	192.578622	4.506778
1.816822	201.036077	4.511782
2.145164	199.516781	4.516787
2.601175	203.325645	4.521792
2.308122	199.373709	4.526797
2.142649	185.694552	4.531802
2.197217	201.131590	4.536806
2.374805	192.962723	4.541811
2.023732	192.488485	4.546816
2.084858	196.071177	4.551821
2.589375	206.501031	4.556826
2.193722	198.734103	4.561830
2.310914	205.157371	4.566835
2.290342	204.438112	4.571840
2.301658	208.812456	4.576845
2.188452	201.331416	4.581850
2.081715	213.312808	4.586854
2.390740	198.525862	4.591859
2.320938	198.199986	4.596864
2.079070	202.726661	4.601869
2.367671	200.016363	4.606874
2.236160	209.077029	4.611878
2.489601	193.596457	4.616883
2.416714	209.137633	4.621888
2.121752	205.840783	4.626893
2.681441	208.473518	4.631898
2.299528	214.108050	4.636902
2.463953	198.539582	4.641907
2.563470	216.071243	4.646912
2.298857	204.369612	4.651917
2.496014	203.968839	4.656922
2.161599	215.833167	4.661926
2.403781	214.214359	4.666931
2.540646	215.136546	4.671936
2.577147	221.168572	4.676941
2.886477	221.752187	4.681946
2.517624	224.069957	4.686950
2.567421	212.835484	4.691955
2.509220	225.155933	4.696960
2.587431	223.960024	4.701965
3.112707	229.323890	4.706970
2.405914	223.487348	4.711974
2.722226	219.887928	4.716979
2.757298	221.530247	4.721984
2.611002	232.683177	4.726989
3.053797	226.455699	4.731994
2.799209	232.023223	4.736998
2.473575	211.234406	4.742003
2.767413	217.379582	4.747008
2.515069	216.510784	4.752013
3.061400	221.474477	4.757018
2.665800	225.459003	4.762022
3.144970	221.846481	4.767027
2.883603	221.054842	4.772032
2.617981	205.762439	4.777037
3.255006	210.833966	4.782042
2.818675	218.165179	4.787046
2.632075	204.354537	4.792051
2.694946	212.968536	4.797056
2.890594	211.016763	4.802061
2.795575	213.716949	4.807066
3.243220	222.369080	4.812070
2.882270	230.461494	4.817075
2.592091	221.834808	4.822080
2.682592	226.483256	4.827085
3.080643	220.728431	4.832090
3.172060	229.587121	4.837094
3.199959	225.786948	4.842099
3.148931	230.435009	4.847104
2.856635	235.089795	4.852109
3.253242	223.847231	4.857114
3.291430	234.200462	4.862118
2.938679	225.712859	4.867123
3.151310	233.528963	4.872128
2.962044	232.232628	4.877133
3.166795	222.245485	4.882138
2.948995	230.920675	4.887142
2.999010	230.869087	4.892147
2.844373	234.831454	4.897152
2.779387	238.721984	4.902157
3.013330	225.601174	4.907162
2.981633	231.342787	4.912166
3.233819	228.319551	4.917171
3.108271	233.621382	4.922176
2.921238	231.340102	4.927181
3.133253	224.897909	4.932186
2.835795	234.974734	4.937190
3.133730	229.957223	4.942195
3.321652	230.597699	4.947200
3.060132	227.798656	4.952205
3.260069	239.178697	4.957210
2.986413	244.054352	4.962214
3.386224	254.023262	4.967219
3.415836	251.464472	4.972224
3.231270	258.076437	4.977229
3.386140	258.904099	4.982234
3.439781	269.990769	4.987238
3.461872	259.319031	4.992243
3.456898	273.184343	4.997248
3.342717	270.857770	5.002253
3.620279	251.135125	5.007258
3.770665	272.348637	5.012262
3.480374	245.019508	5.017267
3.455248	242.085011	5.022272
3.073731	241.682197	5.027277
3.242174	246.409618	5.032282
3.519600	259.515368	5.037286
3.708190	250.028298	5.042291
3.650539	255.437993	5.047296
3.440086	264.493190	5.052301
4.032734	260.529537	5.057306
3.325624	247.972258	5.062310
3.217329	234.329384	5.067315
3.493552	243.980325	5.072320
3.570451	247.970828	5.077325
3.738422	248.297032	5.082330
3.133459	262.791262	5.087334
3.450519	255.821552	5.092339
3.698166	258.557361	5.097344
3.797510	257.164199	5.102349
3.653951	262.730256	5.107354
3.502342	252.988836	5.112358
3.655701	258.025473	5.117363
3.598710	263.872005	5.122368
3.475038	264.732972	5.127373
3.884846	257.956688	5.132378
3.215827	259.486190	5.137382
3.376576	253.964820	5.142387
3.660596	256.439890	5.147392
3.291810	262.810506	5.152397
3.551508	257.681807	5.157402
3.781390	289.253227	5.162406
4.055072	280.527606	5.167411
4.051006	282.464078	5.172416
3.721948	284.447943	5.177421
3.680578	273.504727	5.182426
3.767227	289.107422	5.187430
3.995531	284.053159	5.192435
4.058307	286.894403	5.197440
3.918409	289.951850	5.202445
4.197723	294.761001	5.207450
3.975144	273.575640	5.212454
3.921302	253.702949	5.217459
3.976670	259.934708	5.222464
3.806638	256.358430	5.227469
3.889243	271.692448	5.232474
3.806234	276.024587	5.237478
3.867098	286.880208	5.242483
4.341927	284.252968	5.247488
3.979181	290.264873	5.252493
4.305917	279.831246	5.257498
3.852808	281.237266	5.262502
3.901758	285.678319	5.267507
3.948004	283.982771	5.272512
3.850826	297.789844	5.277517
4.215116	282.585547	5.282522
3.994371	286.446484	5.287526
4.131869	288.330065	5.292531
4.139651	284.787732	5.297536
3.976796	286.167393	5.302541
4.170640	291.908457	5.307546
3.969024	290.453547	5.312550
4.223306	298.487833	5.317555
4.327372	291.540086	5.322560
3.801831	288.677028	5.327565
4.167775	286.476906	5.332570
3.899064	295.692099	5.337574
4.234526	292.344028	5.342579
4.143712	283.075954	5.347584
3.820897	296.070496	5.352589
3.967785	282.127328	5.357594
4.432517	307.111931	5.362598
4.509651	316.024135	5.367603
4.298276	298.171346	5.372608
4.475042	307.081287	5.377613
4.103437	285.578597	5.382618
4.278310	304.713486	5.387622
4.561814	299.496390	5.392627
4.300035	306.202428	5.397632
4.497919	312.059344	5.402637
4.511009	319.342875	5.407642
4.551412	315.306701	5.412646
4.377689	299.891482	5.417651
4.374402	300.646529	5.422656
4.160660	305.888968	5.427661
4.702110	310.581405	5.432666
4.475899	314.726196	5.437670
4.525977	321.617182	5.442675
4.458267	313.642690	5.447680
4.595705	322.494026	5.452685
4.675961	314.203358	5.457690
4.877559	315.872429	5.462694
4.730885	298.331551	5.467699
4.418538	279.313282	5.472704
4.310379	285.931673	5.477709
4.241837	288.491451	5.482714
4.603414	301.065883	5.487718
4.293432	312.364603	5.492723
4.446055	299.328200	5.497728
4.606476	315.413586	5.502733
4.888190	306.672910	5.507738
4.867589	313.512630	5.512742
4.819231	317.314207	5.517747
5.085943	310.515870	5.522752
4.731337	320.183895	5.527757
4.900967	310.642996	5.532762
4.713954	321.441640	5.537766
4.802517	308.239617	5.542771
4.883973	312.681620	5.547776
4.540476	306.319553	5.552781
4.488222	311.225529	5.557786
4.357427	317.120485	5.562790
4.495317	315.211886	5.567795
4.736645	317.451033	5.572800
4.714310	320.681338	5.577805
4.944183	310.053363	5.582810
4.860669	321.705834	5.587814
4.916958	317.106375	5.592819
4.616140	316.919103	5.597824
4.246475	317.263221	5.602829
5.194564	315.415972	5.607834
4.839909	321.319610	5.612838
5.026288	303.993115	5.617843
5.006804	312.977813	5.622848
4.802117	319.850917	5.627853
5.051061	311.349466	5.632858
4.893840	316.026842	5.637862
4.963261	317.116451	5.642867
4.908574	314.355131	5.647872
5.158846	319.514088	5.652877
5.087109	317.800347	5.657882
4.669756	323.235373	5.662886
5.032136	324.040586	5.667891
5.547888	345.603735	5.672896
5.292491	326.487305	5.677901
5.230706	319.929314	5.682906
4.697662	325.230741	5.687910
4.937117	320.552079	5.692915
5.133238	314.370164	5.697920
5.283588	335.321938	5.702925
5.442119	328.045923	5.707930
4.841060	318.386135	5.712934
4.984961	335.675009	5.717939
5.390227	336.586688	5.722944
5.045632	344.358294	5.727949
5.451494	337.810522	5.732954
5.613816	339.183608	5.737958
5.164118	329.979154	5.742963
4.934867	319.860340	5.747968
5.251940	336.863699	5.752973
5.254468	333.284537	5.757978
5.495735	342.812670	5.762982
5.130274	343.341567	5.767987
5.387089	338.426611	5.772992
5.283822	341.789470	5.777997
4.953805	339.947537	5.783002
5.211097	344.223262	5.788006
5.614786	340.009646	5.793011
5.384456	341.439629	5.798016
5.135700	352.877723	5.803021
5.431242	345.254285	5.808026
5.010818	344.147971	5.813030
5.334447	340.502227	5.818035
5.321901	343.772355	5.823040
4.658419	346.339202	5.828045
5.309143	341.860617	5.833050
5.797646	360.575563	5.838054
5.577471	354.774475	5.843059
5.402762	331.577229	5.848064
5.367136	352.227585	5.853069
5.431895	350.945593	5.858074
5.607289	368.652237	5.863078
5.558186	369.904784	5.868083
6.129450	371.166194	5.873088
5.751033	347.827078	5.878093
5.678327	341.344380	5.883098
5.358049	341.856241	5.888102
5.678546	337.679558	5.893107
5.857648	342.092214	5.898112
5.918580	337.655552	5.903117
5.674283	343.616334	5.908122
5.423886	331.156061	5.913126
5.336936	341.298303	5.918131
5.726318	346.447105	5.923136
5.552934	339.791627	5.928141
5.924865	345.477730	5.933146
5.364716	349.788998	5.938150
6.165947	358.418588	5.943155
5.858622	348.257805	5.948160
5.507143	344.071215	5.953165
5.778051	348.506289	5.958170
5.787818	368.342261	5.963174
5.983808	358.040583	5.968179
5.992462	354.135727	5.973184
5.779223	351.257847	5.978189
5.633186	339.307439	5.983194
5.891160	342.233146	5.988198
6.283281	360.185923	5.993203
6.159206	341.343839	5.998208
5.847392	346.938816	6.003213
5.955733	339.591771	6.008218
5.894410	336.970451	6.013222
5.697945	339.860169	6.018227
5.593375	333.684232	6.023232
5.379079	351.597417	6.028237
6.179656	354.341511	6.033242
6.171613	359.903755	6.038246
5.995129	353.307879	6.043251
5.836281	345.257076	6.048256
5.684612	344.557600	6.053261
5.791709	336.856786	6.058266
5.538994	354.292417	6.063270
5.676393	363.044338	6.068275
6.092732	368.928315	6.073280
6.046479	369.860450	6.078285
6.357635	368.165707	6.083290
5.715396	360.928088	6.088294
5.399393	348.885104	6.093299
5.818070	353.303257	6.098304
5.777509	359.842930	6.103309
6.484235	364.705679	6.108314
6.139150	353.547409	6.113318
5.719672	348.606486	6.118323
6.215579	345.551534	6.123328
6.050901	343.134640	6.128333
6.170152	337.167564	6.133338
5.875941	348.074803	6.138342
5.874411	337.692819	6.143347
6.082130	339.044394	6.148352
5.886026	343.625010	6.153357
6.040062	341.401790	6.158362
5.691183	346.388564	6.163366
5.625506	341.569322	6.168371
5.857820	338.118519	6.173376
5.672148	337.128696	6.178381
5.973406	334.758716	6.183386
5.771685	328.501364	6.188390
5.713185	328.797712	6.193395
5.974094	339.589335	6.198400
5.333653	333.148273	6.203405
5.532012	337.007838	6.208410
6.058149	343.477927	6.213414
5.773250	343.154740	6.218419
6.105799	342.627212	6.223424
5.986880	351.474561	6.228429
5.782323	327.926105	6.233434
5.611910	338.836063	6.238438
5.923230	350.004514	6.243443
5.810154	356.076407	6.248448
6.092994	362.902802	6.253453
6.037127	348.496545	6.258458
5.981585	340.794587	6.263462
5.712720	341.602304	6.268467
5.672586	332.943607	6.273472
5.600662	345.744208	6.278477
6.035189	352.694897	6.283482
6.171430	366.080279	6.288486
6.333712	357.440109	6.293491
6.348556	338.559089	6.298496
5.798517	341.622763	6.303501
6.175813	339.019623	6.308506
5.938791	330.759673	6.313510
5.880119	339.793384	6.318515
6.157731	329.595340	6.323520
5.859894	346.474701	6.328525
5.670570	330.709730	6.333530
5.489696	344.678462	6.338534
5.783170	339.228950	6.343539
5.971266	338.490986	6.348544
5.892220	346.571996	6.353549
5.809016	339.684474	6.358554
6.064710	340.146435	6.363558
5.860185	340.216625	6.368563
5.909830	342.806209	6.373568
5.789425	336.154901	6.378573
5.958667	335.359380	6.383578
5.792944	351.316583	6.388582
5.839765	343.314664	6.393587
6.005454	337.986208	6.398592
6.115880	342.032756	6.403597
6.071259	331.215426	6.408602
6.282787	345.027168	6.413606
6.111488	340.008437	6.418611
6.142224	340.226011	6.423616
5.997454	340.108647	6.428621
5.816924	315.495001	6.433626
5.888561	316.745842	6.438630
5.724192	322.017321	6.443635
5.859289	309.311341	6.448640
6.048630	332.112278	6.453645
6.065080	327.269603	6.458650
5.791600	318.919396	6.463654
6.112631	319.531763	6.468659
6.088292	314.764497	6.473664
5.796055	316.603868	6.478669
5.849726	311.654419	6.483674
5.740737	317.770509	6.488678
5.755015	320.214891	6.493683
5.814415	317.460368	6.498688
5.655747	316.332109	6.503693
5.909448	312.298472	6.508698
6.064794	322.163395	6.513702
5.781394	315.729930	6.518707
5.733492	312.442741	6.523712
5.789495	320.590407	6.528717
5.957819	336.376768	6.533722
6.027352	325.624829	6.538726
5.788812	321.743370	6.543731
5.985833	317.077048	6.548736
5.749183	314.488750	6.553741
5.969614	319.288106	6.558746
5.845058	320.844743	6.563750
5.598691	320.188343	6.568755
6.104793	326.471528	6.573760
5.973879	337.662243	6.578765
5.622952	326.402948	6.583770
5.641237	323.736609	6.588774
5.721416	335.871200	6.593779
6.226990	328.403269	6.598784
5.764372	345.330775	6.603789
6.117967	332.904070	6.608794
6.095050	335.895629	6.613798
5.763447	325.420906	6.618803
5.957190	312.927898	6.623808
5.562679	313.015277	6.628813
5.687984	321.860824	6.633818
5.770180	333.659258	6.638822
5.898354	336.559058	6.643827
6.108215	339.143080	6.648832
6.032941	337.191668	6.653837
5.983147	327.335707	6.658842
5.988584	325.747625	6.663846
5.643350	314.177817	6.668851
5.794951	314.843339	6.673856
6.070501	333.994480	6.678861
6.140686	328.010754	6.683866
6.067277	316.996441	6.688870
5.509867	306.123482	6.693875
5.840165	317.321330	6.698880
5.694410	315.177745	6.703885
6.235681	326.382269	6.708890
6.032230	312.193010	6.713894
5.963003	318.828363	6.718899
5.784004	301.650548	6.723904
5.536286	319.832629	6.728909
5.711949	311.865274	6.733914
5.759723	314.891515	6.738918
5.845413	328.270024	6.743923
6.129367	330.849791	6.748928
5.814677	327.691826	6.753933
5.835411	332.348284	6.758938
6.194999	325.554126	6.763942
5.791469	322.993996	6.768947
5.744149	310.830874	6.773952
5.937479	316.712715	6.778957
6.030841	318.468929	6.783962
5.805727	313.434141	6.788966
5.466773	322.893687	6.793971
6.151622	321.081652	6.798976
5.867792	326.495009	6.803981
5.632795	316.446403	6.808986
6.130380	324.279491	6.813990
5.944535	330.108670	6.818995
5.902349	311.604501	6.824000
5.629382	315.111121	6.829005
5.641814	321.472629	6.834010
5.867894	339.778976	6.839014
5.852483	341.153711	6.844019
5.904187	326.871663	6.849024
5.920519	342.356696	6.854029
5.971107	333.762719	6.859034
6.244582	336.549521	6.864038
5.859885	331.040619	6.869043
5.678772	312.269360	6.874048
5.687001	320.521307	6.879053
6.031765	328.830902	6.884058
6.233733	329.302531	6.889062
5.673292	322.860980	6.894067
5.892639	317.308298	6.899072
5.964294	307.977351	6.904077
5.955667	307.228489	6.909082
6.035948	311.853791	6.914086
5.953705	317.422066	6.919091
5.802682	313.506119	6.924096
5.646529	320.402279	6.929101
5.724490	305.034352	6.934106
5.994888	316.318949	6.939110
5.838892	318.338938	6.944115
5.869765	319.788104	6.949120
5.878551	311.685545	6.954125
5.824585	314.228514	6.959130
6.186646	308.643865	6.964134
5.718005	312.948585	6.969139
6.036023	315.247570	6.974144
5.839998	305.637368	6.979149
5.842448	314.810032	6.984154
6.075691	319.385591	6.989158
5.928955	312.172462	6.994163
5.899943	320.082309	6.999168
5.713230	314.913711	7.004173
5.910425	316.219373	7.009178
5.292717	320.430835	7.014182
5.516496	334.707183	7.019187
6.435572	328.852898	7.024192
5.826936	336.906092	7.029197
5.509673	321.654761	7.034202
5.927931	321.910995	7.039206
5.833674	341.366640	7.044211
6.251674	338.976085	7.049216
5.939777	331.265294	7.054221
5.790361	316.119121	7.059226
5.834120	322.349666	7.064230
5.718445	330.439976	7.069235
6.270908	331.244854	7.074240
5.623997	325.010561	7.079245
5.950653	331.171670	7.084250
5.908890	331.376659	7.089254
5.717297	323.685946	7.094259
6.093025	329.536269	7.099264
5.724745	327.298639	7.104269
5.839690	329.133467	7.109274
5.925451	327.054422	7.114278
5.744678	329.036676	7.119283
6.030109	340.252313	7.124288
5.764279	339.341441	7.129293
5.520993	338.492843	7.134298
6.182779	334.845875	7.139302
6.100476	337.148371	7.144307
6.051925	331.966308	7.149312
5.629570	324.029108	7.154317
5.537305	316.639260	7.159322
6.108565	324.941513	7.164326
5.802223	333.600217	7.169331
6.158674	327.880344	7.174336
5.897189	327.580912	7.179341
5.992467	326.273950	7.184346
5.878386	319.316365	7.189350
5.822216	322.160007	7.194355
5.871451	317.214742	7.199360
5.817500	322.614576	7.204365
5.739541	314.496162	7.209370
5.698672	321.182373	7.214374
5.838327	339.467880	7.219379
6.033327	338.982320	7.224384
5.951151	343.971091	7.229389
5.863630	330.191317	7.234394
6.002160	324.916384	7.239398
5.605699	324.920327	7.244403
5.952841	333.305003	7.249408
6.089094	326.521607	7.254413
5.858748	324.778139	7.259418
5.852638	311.900845	7.264422
5.692011	314.380444	7.269427
6.009440	316.291614	7.274432
5.810615	324.356693	7.279437
5.849260	330.820618	7.284442
5.958949	323.668992	7.289446
5.794605	329.222722	7.294451
6.105315	326.122907	7.299456
6.058064	325.209260	7.304461
5.620114	316.594016	7.309466
5.719799	325.879363	7.314470
5.900993	335.119183	7.319475
5.817437	316.771505	7.324480
5.938035	336.586852	7.329485
5.943184	331.276937	7.334490
5.920703	317.938268	7.339494
5.914449	322.867920	7.344499
5.771090	323.971185	7.349504
5.859846	324.549425	7.354509
5.672409	325.754881	7.359514
5.956575	333.609430	7.364518
5.837387	337.267433	7.369523
6.029056	336.232912	7.374528
6.077942	338.532671	7.379533
5.816608	324.252733	7.384538
5.961502	314.132668	7.389542
5.413319	328.938898	7.394547
6.011778	323.214846	7.399552
5.860842	338.996649	7.404557
5.952104	334.818683	7.409562
5.881033	325.539428	7.414566
5.970649	332.171820	7.419571
5.910904	325.399604	7.424576
5.711805	317.089591	7.429581
5.792898	322.722824	7.434586
5.846523	337.352067	7.439590
5.862774	339.526995	7.444595
5.900852	330.538196	7.449600
5.924052	341.054292	7.454605
6.009080	337.686824	7.459610
6.291951	321.119206	7.464614
6.132868	312.143663	7.469619
5.953265	308.354575	7.474624
5.816045	314.867879	7.479629
5.764982	313.172821	7.484634
5.716950	308.644075	7.489638
5.660438	320.801342	7.494643
5.737676	315.485142	7.499648
5.508341	323.563254	7.504653
5.969935	328.999240	7.509658
6.165753	345.184765	7.514662
5.726709	334.550112	7.519667
5.790433	316.927088	7.524672
5.500887	336.278953	7.529677
5.738846	337.705540	7.534682
6.025421	335.033931	7.539686
5.961811	339.715575	7.544691
6.268062	334.577974	7.549696
5.983338	341.665177	7.554701
5.468523	331.818480	7.559706
6.073315	327.054286	7.564710
5.889714	339.716376	7.569715
6.006931	335.391169	7.574720
6.018441	324.601465	7.579725
5.509471	326.207817	7.584730
5.807966	328.182691	7.589734
5.617849	346.720803	7.594739
6.115699	336.721259	7.599744
5.906395	340.995363	7.604749
5.761803	350.842290	7.609754
6.159924	332.197163	7.614758
5.725077	345.745566	7.619763
5.873228	338.046549	7.624768
5.838282	346.313439	7.629773
5.988841	345.839268	7.634778
6.009639	346.881272	7.639782
5.925913	345.103706	7.644787
5.865304	329.087204	7.649792
6.000615	322.613449	7.654797
5.738261	332.745801	7.659802
5.862304	321.915995	7.664806
5.910871	333.335624	7.669811
5.918870	335.539439	7.674816
5.870402	330.872542	7.679821
6.013552	338.585642	7.684826
6.091157	319.920787	7.689830
5.622244	322.880189	7.694835
5.996506	314.958445	7.699840
6.026771	319.247016	7.704845
6.104845	311.384578	7.709850
6.045221	309.546799	7.714854
5.655913	319.181885	7.719859
5.942832	309.752915	7.724864
5.872963	318.800204	7.729869
5.402390	324.116365	7.734874
5.728738	311.873734	7.739878
5.894801	320.530821	7.744883
5.952002	315.029698	7.749888
5.938367	312.274814	7.754893
5.922278	321.392931	7.759898
6.010833	319.237558	7.764902
6.013855	315.071812	7.769907
6.226770	311.589099	7.774912
5.747446	312.731407	7.779917
5.554061	320.390506	7.784922
5.729345	314.596001	7.789926
5.438855	319.386855	7.794931
6.265875	319.803533	7.799936
5.901331	321.020597	7.804941
5.819123	321.739951	7.809946
6.204034	309.836884	7.814950
5.631302	318.501421	7.819955
5.600633	308.294256	7.824960
6.098465	314.473043	7.829965
5.864316	319.610930	7.834970
5.904511	313.811324	7.839974
5.737129	315.172695	7.844979
5.938366	311.473587	7.849984
6.161752	316.591604	7.854989
5.870373	318.091755	7.859994
6.188471	318.029506	7.864998
6.047845	321.547505	7.870003
6.161377	323.445805	7.875008
6.020042	316.684412	7.880013
6.157435	318.249061	7.885018
6.308329	310.872603	7.890022
5.880328	318.206137	7.895027
6.013319	320.204217	7.900032
6.035369	318.071180	7.905037
5.764668	317.503843	7.910042
5.962624	308.702127	7.915046
5.840341	325.044477	7.920051
5.804943	314.006324	7.925056
5.965186	313.252641	7.930061
5.829618	317.581638	7.935066
5.869192	311.444241	7.940070
5.775470	313.138240	7.945075
6.034043	316.113466	7.950080
5.729857	317.828927	7.955085
5.928004	309.216499	7.960090
5.858283	325.237326	7.965094
5.475770	315.942656	7.970099
5.531223	312.609974	7.975104
5.762662	320.078213	7.980109
5.711667	314.760908	7.985114
6.091830	308.452985	7.990118
5.779769	319.524162	7.995136
5.958579	319.697805	8.000154
5.925912	316.178662	8.005171
5.894568	320.385476	8.010189
6.120314	312.128883	8.015206
5.834258	327.429622	8.020224
6.161392	314.690115	8.025242
5.821274	319.709108	8.030259
6.069787	316.513792	8.035277
6.142122	321.061171	8.040294
5.735053	324.482623	8.045312
6.046189	317.639854	8.050330
5.859652	316.775193	8.055347
6.165755	319.790663	8.060365
6.129045	316.496450	8.065382
5.670297	314.959607	8.070400
6.069979	322.771854	8.075418
6.137619	325.978963	8.080435
6.044149	326.221120	8.085453
6.218844	318.592707	8.090470
6.120927	314.248406	8.095488
5.783863	301.242376	8.100506
5.896887	304.272332	8.105523
5.867354	318.017516	8.110541
5.981889	307.752676	8.115558
6.040282	322.577190	8.120576
6.084210	314.338932	8.125594
6.390729	312.577418	8.130611
5.828531	308.438261	8.135629
5.842877	301.318435	8.140646
6.087869	316.694756	8.145664
6.049727	311.901894	8.150682
6.335702	316.863967	8.155699
5.789069	308.440787	8.160717
5.851928	304.856265	8.165734
5.931176	312.645394	8.170752
5.859443	317.436512	8.175770
5.916844	319.251225	8.180787
5.735737	318.452876	8.185805
5.954526	307.018894	8.190822
6.108610	312.754270	8.195840
6.039195	314.511708	8.200858
6.198106	309.425317	8.205875
5.514744	321.550976	8.210893
6.041590	320.596372	8.215910
6.197475	315.628465	8.220928
6.123374	318.743961	8.225946
6.122002	317.413264	8.230963
5.971990	326.445930	8.235981
6.275124	308.119678	8.240998
6.145318	315.087439	8.246016
6.303651	321.083871	8.251034
6.091043	313.147006	8.256051
5.574325	322.084003	8.261069
5.955655	319.261141	8.266086
6.135412	313.054912	8.271104
6.050088	315.789177	8.276122
6.091621	314.688543	8.281139
6.312274	332.969748	8.286157
6.298830	330.312789	8.291174
6.046104	331.160764	8.296192
6.364173	332.953362	8.301210
6.022088	327.077307	8.306227
5.901712	342.884720	8.311245
6.561838	333.152206	8.316262
6.563872	341.336015	8.321280
5.989356	319.013947	8.326298
6.150967	310.952656	8.331315
6.057898	337.066302	8.336333
6.278075	324.166842	8.341350
6.454454	341.899884	8.346368
6.460720	338.568749	8.351386
6.488337	312.615959	8.356403
5.795235	328.650553	8.361421
6.281923	328.091674	8.366438
6.177957	334.826090	8.371456
5.980895	344.486487	8.376474
6.637656	353.888789	8.381491
6.388207	345.145965	8.386509
5.957095	328.851244	8.391526
5.903827	340.914810	8.396544
6.379947	337.547064	8.401562
6.323643	340.653031	8.406579
6.134289	355.541052	8.411597
5.949230	345.577513	8.416614
6.151728	341.442166	8.421632
6.210579	349.033842	8.426650
6.427251	344.316847	8.431667
6.270180	347.614430	8.436685
6.313985	344.188132	8.441702
6.268387	343.673524	8.446720
6.176280	351.421418	8.451738
6.329587	345.255366	8.456755
5.879686	347.858685	8.461773
6.370784	348.752111	8.466790
6.395027	350.242751	8.471808
6.276600	357.515082	8.476826
6.537766	342.166642	8.481843
6.387130	355.332986	8.486861
6.507260	346.639889	8.491878
6.330738	347.189113	8.496896
6.759625	344.567595	8.501914
6.552161	344.306754	8.506931
6.227689	342.049148	8.511949
6.211133	342.033077	8.516966
6.020320	341.905085	8.521984
6.497238	347.856555	8.527002
6.683759	339.535775	8.532019
6.240328	354.028377	8.537037
6.410886	335.121473	8.542054
6.690493	345.426368	8.547072
6.595894	350.888355	8.552090
6.704600	337.491964	8.557107
6.474132	342.578161	8.562125
6.329806	344.748781	8.567143
6.599032	349.247886	8.572160
6.494884	343.019187	8.577178
6.658141	334.060463	8.582195
6.210171	348.092000	8.587213
6.482513	342.766526	8.592231
6.382594	342.093215	8.597248
6.302901	349.851751	8.602266
6.431041	341.782593	8.607283
6.590179	362.989709	8.612301
6.821813	357.615063	8.617319
6.482584	354.268495	8.622336
6.247557	347.281668	8.627354
6.481030	358.738732	8.632371
6.559470	374.613301	8.637389
6.947448	371.928179	8.642407
6.478170	356.675636	8.647424
6.650093	363.455398	8.652442
6.717314	352.943284	8.657459
6.121733	352.808083	8.662477
6.237845	363.281021	8.667495
6.653875	371.687117	8.672512
6.505442	379.920217	8.677530
6.911555	369.696306	8.682547
6.544556	388.965542	8.687565
6.722495	369.724179	8.692583
6.496983	379.104025	8.697600
6.526241	380.652390	8.702618
6.759615	380.935299	8.707635
6.641919	383.749220	8.712653
6.824513	373.404797	8.717671
6.889279	381.445908	8.722688
6.600218	380.403050	8.727706
6.804302	374.502258	8.732723
6.736335	377.734148	8.737741
6.608055	375.051680	8.742759
6.641233	366.832292	8.747776
6.687113	377.808473	8.752794
7.013739	372.379747	8.757811
6.532007	373.125539	8.762829
6.616301	369.442205	8.767847
6.949657	369.767141	8.772864
6.597442	365.679273	8.777882
6.673739	366.776159	8.782899
6.820038	375.695138	8.787917
6.869454	370.945453	8.792935
6.807127	358.293690	8.797952
6.524322	359.734799	8.802970
6.674692	358.817117	8.807987
6.502925	370.186368	8.813005
6.787683	373.004434	8.818023
6.755604	371.307332	8.823040
6.844323	387.716321	8.828058
7.347266	369.230921	8.833075
6.797347	365.145613	8.838093
6.609614	353.969777	8.843111
6.704440	357.138253	8.848128
6.855732	370.774387	8.853146
7.046550	367.588399	8.858163
6.811791	361.470233	8.863181
6.517259	358.189096	8.868199
6.968011	370.929469	8.873216
6.629472	375.787820	8.878234
7.084584	377.137886	8.883251
6.932810	383.574285	8.888269
6.847031	375.513005	8.893287
6.848048	382.845415	8.898304
6.696045	379.260859	8.903322
6.918845	378.180550	8.908339
7.185394	376.369839	8.913357
7.057603	379.006234	8.918375
6.723890	354.702018	8.923392
6.300230	359.812766	8.928410
6.229972	370.502884	8.933427
6.895022	379.629186	8.938445
6.575994	378.533223	8.943463
6.604895	371.849350	8.948480
6.550349	387.285770	8.953498
6.321199	380.325314	8.958515
7.361547	394.875445	8.963533
7.151440	392.237985	8.968551
6.936566	382.626814	8.973568
6.843029	380.577444	8.978586
7.246019	389.124061	8.983603
6.845477	381.696364	8.988621
6.838352	385.414651	8.993639
7.046239	377.421253	8.998656
6.947109	389.109349	9.003674
7.029507	387.661872	9.008691
7.307875	386.127986	9.013709
7.227750	384.331955	9.018727
7.128632	365.856898	9.023744
7.065067	378.049825	9.028762
7.104240	366.808537	9.033779
7.178597	377.862080	9.038797
6.981995	380.762056	9.043815
7.408386	369.325112	9.048832
7.087871	382.601522	9.053850
7.277192	372.592826	9.058867
7.135549	372.132565	9.063885
6.992302	379.047470	9.068903
7.400374	382.127875	9.073920
7.243804	382.591439	9.078938
7.373796	386.869916	9.083955
7.553651	374.455027	9.088973
7.303194	376.329871	9.093991
7.253948	357.576562	9.099008
6.449133	360.237353	9.104026
6.856008	367.999921	9.109043
7.292104	370.407037	9.114061
6.852589	366.363707	9.119079
7.081410	374.980822	9.124096
6.803502	380.168256	9.129114
6.741093	374.021998	9.134131
6.708425	378.319972	9.139149
6.821329	379.618935	9.144167
7.009321	385.180661	9.149184
7.168052	392.488882	9.154202
7.121101	403.754281	9.159219
7.293453	399.358011	9.164237
7.069149	407.704626	9.169255
7.487002	396.921592	9.174272
7.182556	395.740262	9.179290
7.098924	385.224124	9.184307
7.414744	383.727643	9.189325
7.239931	389.821174	9.194343
7.353913	375.609582	9.199360
7.321286	376.974613	9.204378
7.126295	368.820483	9.209395
7.015542	369.567751	9.214413
7.190745	388.127734	9.219431
7.616298	386.253746	9.224448
7.316208	391.871236	9.229466
6.962057	380.029034	9.234483
7.496459	388.687175	9.239501
7.120664	385.873597	9.244519
7.326266	386.605685	9.249536
7.332865	403.823763	9.254554
7.642432	410.845606	9.259571
7.402775	386.626169	9.264589
7.310786	380.316918	9.269607
7.099443	379.392686	9.274624
7.094824	388.885117	9.279642
7.511383	403.029983	9.284659
7.618634	396.945226	9.289677
7.136477	398.332194	9.294695
7.348231	395.964219	9.299712
7.393751	404.294780	9.304730
7.452695	409.513941	9.309747
7.699730	399.468137	9.314765
7.381001	388.665424	9.319783
7.263733	366.904596	9.324800
7.184096	385.106283	9.329818
7.357656	400.571936	9.334835
7.450988	407.441264	9.339853
7.361044	401.382696	9.344871
7.499034	398.965605	9.349888
7.456914	405.463305	9.354906
7.564420	408.402382	9.359923
7.456360	404.909258	9.364941
7.304801	409.743806	9.369959
7.691247	402.045425	9.374976
7.608455	396.954075	9.379994
7.198700	386.737643	9.385011
7.539098	385.325172	9.390029
7.379574	396.805781	9.395047
7.659840	397.500045	9.400064
7.635332	410.489523	9.405082
7.514769	401.376426	9.410099
7.115767	393.847702	9.415117
7.310348	408.567429	9.420135
7.779898	399.369213	9.425152
7.872326	412.552021	9.430170
7.481133	409.618273	9.435187
7.699214	401.653191	9.440205
7.479067	392.853343	9.445223
7.674651	393.612673	9.450240
7.314664	389.973822	9.455258
7.342339	406.521829	9.460275
7.641319	409.007405	9.465293
7.723261	406.177322	9.470311
7.611573	400.844439	9.475328
7.681459	394.907068	9.480346
7.620296	409.841463	9.485363
7.516521	395.708546	9.490381
7.470259	406.887631	9.495399
7.534871	402.082091	9.500416
7.398209	401.890732	9.505434
7.646615	410.344133	9.510451
7.435992	396.524478	9.515469
7.633619	405.193508	9.520487
7.629208	400.174717	9.525504
7.815025	402.333790	9.530522
7.831663	402.108930	9.535539
7.993567	399.827030	9.540557
7.737840	402.984858	9.545575
7.709098	396.550804	9.550592
7.870613	402.673585	9.555610
7.917213	401.871060	9.560627
8.027694	392.485978	9.565645
7.810679	401.750777	9.570663
7.568790	373.734797	9.575680
7.600700	378.282969	9.580698
7.695234	393.857127	9.585715
7.687333	398.911975	9.590733
7.462240	399.361081	9.595751
7.645186	394.703669	9.600768
7.823680	403.014518	9.605786
7.650019	403.373941	9.610803
7.805890	392.048500	9.615821
7.599095	402.415608	9.620839
7.362716	405.928727	9.625856
7.608952	400.602332	9.630874
7.680636	405.818205	9.635891
7.649523	404.092205	9.640909
7.607559	401.261737	9.645927
7.690813	405.534461	9.650944
7.854096	400.525352	9.655962
7.560257	407.197988	9.660979
8.107885	414.481019	9.665997
7.833165	411.964151	9.671015
7.690519	410.471202	9.676032
8.157251	420.537000	9.681050
7.924273	419.693588	9.686067
7.838883	398.121403	9.691085
7.913801	398.277774	9.696103
7.953036	397.789294	9.701120
8.034664	401.017232	9.706138
7.921384	394.268478	9.711155
7.931109	394.628199	9.716173
7.934985	400.978169	9.721191
8.122238	398.091125	9.726208
8.004204	397.906528	9.731226
7.884074	404.727683	9.736243
7.971077	393.271428	9.741261
7.751423	390.264169	9.746279
7.815905	404.638344	9.751296
8.253300	399.657445	9.756314
7.937400	404.983913	9.761331
8.033623	393.436193	9.766349
7.900752	395.953475	9.771367
7.639513	396.300211	9.776384
8.081734	405.061764	9.781402
7.918889	416.468346	9.786419
8.330435	413.808253	9.791437
8.253203	433.310014	9.796455
7.654658	417.081836	9.801472
8.091785	419.366177	9.806490
8.160017	426.941187	9.811507
8.213551	418.504574	9.816525
8.259786	423.999110	9.821543
8.230775	410.792898	9.826560
8.224040	401.160407	9.831578
7.754954	399.329263	9.836595
8.107559	401.914516	9.841613
7.950168	410.160625	9.846631
8.148273	416.511567	9.851648
8.573038	411.687935	9.856666
7.948890	397.725047	9.861683
7.985737	403.565443	9.866701
8.345691	418.623129	9.871719
8.274733	416.655733	9.876736
8.270839	388.363143	9.881754
8.020871	394.280848	9.886771
8.035461	400.189278	9.891789
8.526206	417.736628	9.896807
8.515619	402.295959	9.901824
8.427976	393.867142	9.906842
8.035101	381.198838	9.911859
8.092395	387.482211	9.916877
8.099049	390.581031	9.921895
8.159484	384.926957	9.926912
8.429651	383.379174	9.931930
8.102016	391.970072	9.936947
8.162012	393.999968	9.941965
8.141156	403.530025	9.946983
8.244912	411.033619	9.952000
8.557296	412.672671	9.957018
8.325204	406.975709	9.962035
8.197219	389.171494	9.967053
8.196580	400.288420	9.972071
8.184840	424.557174	9.977088
8.500368	414.255506	9.982106
8.293820	419.142541	9.987123
8.640876	410.358475	9.992141
8.229559	401.068572	9.997159
8.086474	399.761286	10.002176
8.131812	412.675458	10.007194
8.042920	420.974315	10.012211
8.455005	424.675687	10.017229
8.889351	418.096803	10.022247
8.612301	429.955050	10.027264
8.965319	414.211026	10.032282
8.433482	398.991805	10.037299
8.196329	398.730555	10.042317
8.087830	391.596448	10.047335
7.986632	397.963977	10.052352
8.653872	402.983027	10.057370
8.422197	426.483477	10.062387
8.292453	429.047876	10.067405
7.840953	420.668742	10.072423
8.116638	431.814619	10.077440
8.681768	426.777373	10.082458
9.055879	431.074268	10.087475
8.849952	420.983151	10.092493
8.753256	418.934003	10.097511
8.559617	410.004397	10.102528
8.295456	396.911942	10.107546
8.254862	403.011245	10.112563
8.598913	416.323895	10.117581
8.842365	418.728805	10.122599
8.540469	408.257183	10.127616
8.421454	394.885384	10.132634
8.631992	402.017958	10.137651
8.491519	406.324013	10.142669
8.219684	398.478468	10.147687
8.253831	423.083855	10.152704
8.749388	429.991623	10.157722
8.387898	432.136442	10.162739
8.466859	426.008131	10.167757
8.956582	418.945786	10.172775
8.607058	430.075123	10.177792
8.966924	430.753971	10.182810
9.089001	425.651782	10.187827
8.752234	409.796701	10.192845
8.622947	392.846650	10.197863
8.399618	398.118653	10.202880
8.530336	396.512041	10.207898
8.666569	404.415593	10.212915
8.749372	412.882290	10.217933
8.756589	404.440448	10.222951
8.436005	415.585657	10.227968
8.712587	420.588383	10.232986
8.778003	424.615786	10.238003
8.701537	420.306190	10.243021
8.877892	421.172221	10.248039
8.704944	428.424467	10.253056
8.903297	420.524532	10.258074
8.521712	420.577147	10.263091
8.635761	421.576972	10.268109
8.696496	419.617137	10.273127
8.845402	416.611847	10.278144
8.995765	419.057726	10.283162
8.467092	425.202170	10.288179
8.401995	429.028551	10.293197
8.567753	410.220655	10.298215
8.802448	419.671687	10.303232
8.615489	425.982450	10.308250
8.540651	419.844820	10.313267
8.540130	427.913276	10.318285
8.943872	424.319431	10.323303
8.763037	426.455553	10.328320
9.145908	417.637814	10.333338
9.107388	422.030350	10.338355
8.973336	430.164860	10.343373
8.979920	430.338921	10.348391
8.664583	432.736787	10.353408
8.615556	440.128369	10.358426
8.808844	424.269520	10.363443
8.955281	422.773571	10.368461
9.042515	431.384988	10.373479
8.565811	427.535937	10.378496
8.704541	427.349746	10.383514
8.954283	422.933990	10.388531
8.863562	427.623282	10.393549
9.014169	415.820251	10.398567
8.641145	420.447653	10.403584
8.650493	434.617134	10.408602
9.159915	431.683241	10.413619
9.350524	441.897910	10.418637
9.461271	429.399437	10.423655
8.812160	427.573143	10.428672
9.191683	417.449440	10.433690
8.982198	406.210246	10.438707
8.740259	413.199830	10.443725
8.951409	414.621015	10.448743
9.119464	425.510027	10.453760
9.187781	428.013059	10.458778
9.014018	418.317234	10.463795
9.089077	427.671056	10.468813
8.931731	416.707036	10.473831
9.166387	438.340661	10.478848
9.543138	431.939167	10.483866
9.140779	423.428610	10.488883
8.603266	422.710409	10.493901
9.252947	419.565092	10.498919
9.098744	437.974300	10.503936
9.081519	439.130830	10.508954
9.345041	435.850153	10.513971
8.898363	445.999997	10.518989
9.450594	433.714036	10.524007
8.950776	434.418833	10.529024
9.457035	439.469320	10.534042
9.408673	428.627312	10.539059
8.876751	421.827773	10.544077
9.012410	431.558804	10.549095
9.021489	444.221470	10.554112
9.056559	450.202208	10.559130
9.384845	441.307175	10.564147
9.172334	450.602945	10.569165
9.598203	440.282336	10.574183
9.522268	451.119383	10.579200
9.201752	444.455728	10.584218
9.202386	435.459857	10.589235
9.328249	453.494130	10.594253
9.403054	443.613541	10.599271
8.913157	435.666836	10.604288
9.246233	447.267414	10.609306
9.186833	441.983148	10.614323
9.039476	454.166366	10.619341
9.312282	438.572847	10.624359
9.471712	454.078185	10.629376
9.482530	441.138142	10.634394
9.363352	445.556610	10.639411
9.367765	438.332675	10.644429
9.369527	443.898333	10.649447
9.115795	450.413703	10.654464
9.609116	438.221510	10.659482
9.745984	441.176112	10.664499
9.334438	449.615883	10.669517
9.327045	440.340882	10.674535
9.409421	441.321144	10.679552
9.453724	443.841038	10.684570
9.611733	434.222435	10.689587
9.521709	438.333883	10.694605
9.704480	448.779528	10.699623
9.738523	442.440568	10.704640
9.495479	439.776857	10.709658
9.894433	438.814647	10.714675
8.879036	441.990859	10.719693
9.065334	443.104507	10.724711
9.352601	441.328939	10.729728
9.118880	451.816943	10.734746
9.084809	442.929340	10.739763
9.262075	450.549814	10.744781
9.579627	440.691008	10.749799
9.304764	444.131378	10.754816
9.299107	455.832714	10.759834
9.838470	441.352578	10.764851
9.505758	444.393932	10.769869
9.636025	455.434946	10.774887
9.408449	440.821861	10.779904
9.680060	452.241991	10.784922
9.945212	448.884286	10.789939
9.709870	452.416039	10.794957
9.452855	448.113442	10.799975
9.560329	445.677769	10.804992
8.655225	453.214075	10.810010
9.652580	456.200165	10.815027
10.300145	478.279579	10.820045
10.255381	466.131904	10.825063
9.964035	451.157279	10.830080
9.619062	452.677553	10.835098
9.967787	437.699507	10.840115
9.816382	448.039780	10.845133
9.533763	444.726642	10.850151
9.564516	440.022629	10.855168
9.661137	440.155045	10.860186
9.729016	434.707258	10.865203
9.328515	440.767844	10.870221
9.994258	444.714152	10.875239
10.109225	455.808866	10.880256
10.009430	445.375065	10.885274
9.872406	438.710120	10.890291
9.715014	447.595288	10.895309
10.019071	440.640273	10.900327
9.774708	435.828214	10.905344
9.715377	436.181242	10.910362
9.800517	435.366443	10.915379
9.567340	436.416169	10.920397
9.474456	446.932755	10.925415
9.924245	453.167826	10.930432
9.924717	463.719181	10.935450
10.368973	457.921256	10.940467
9.647862	459.428803	10.945485
9.798368	452.726176	10.950503
9.630779	456.005839	10.955520
9.675302	469.517608	10.960538
10.446292	463.457758	10.965555
10.013193	472.967910	10.970573
10.103768	475.242909	10.975591
10.288165	450.527693	10.980608
9.887242	459.298912	10.985626
10.368758	442.506181	10.990643
9.934902	444.391955	10.995661
9.814770	438.771243	11.000679
10.061702	440.848583	11.005696
9.841390	449.043510	11.010714
9.970025	437.835702	11.015731
10.055934	436.014687	11.020749
9.695611	443.565270	11.025767
9.690844	454.397938	11.030784
9.909356	473.854715	11.035802
10.420612	461.926906	11.040819
10.164862	463.681204	11.045837
10.240151	462.319326	11.050855
10.383805	461.851671	11.055872
9.827708	465.997242	11.060890
10.533319	455.316877	11.065907
10.338557	450.638221	11.070925
10.088613	432.270078	11.075943
10.239070	435.691133	11.080960
9.893521	435.849680	11.085978
10.322920	427.998550	11.090995
10.054200	438.239133	11.096013
9.870404	430.344482	11.101031
10.343243	448.391278	11.106048
9.993095	452.327946	11.111066
10.068487	453.043276	11.116083
10.125219	456.669155	11.121101
10.224326	457.182085	11.126119
10.476487	462.982297	11.131136
10.309990	465.404479	11.136154
10.529308	451.740450	11.141171
10.444039	446.891076	11.146189
10.130778	429.870324	11.151207
10.118278	428.971977	11.156224
9.833005	453.286470	11.161242
10.334390	447.542186	11.166259
10.444737	459.416637	11.171277
10.545658	459.254702	11.176295
10.639237	459.212263	11.181312
10.345779	452.222153	11.186330
10.264190	442.594232	11.191347
10.402976	454.926482	11.196365
10.284449	449.743992	11.201383
10.495210	448.727073	11.206400
10.057693	448.183152	11.211418
10.243625	454.160118	11.216435
10.410541	466.936159	11.221453
10.398945	462.755074	11.226471
10.465358	458.571038	11.231488
10.306574	469.564180	11.236506
10.429441	472.199317	11.241523
10.864326	461.940479	11.246541
10.801179	469.351334	11.251559
10.534662	452.644419	11.256576
10.061096	460.783291	11.261594
10.510562	451.876787	11.266611
10.665608	454.885462	11.271629
10.449120	455.052104	11.276647
10.673136	462.184053	11.281664
10.596399	464.505101	11.286682
10.418371	456.962756	11.291699
10.371864	467.393263	11.296717
10.283285	466.283221	11.301735
10.624180	462.691685	11.306752
10.380480	468.518440	11.311770
10.710638	461.096895	11.316787
10.564515	464.868873	11.321805
10.477377	461.416954	11.326823
10.777558	464.322923	11.331840
10.642329	464.189975	11.336858
10.873544	459.617559	11.341875
10.718372	458.118704	11.346893
10.924781	464.492896	11.351911
10.899036	457.025956	11.356928
10.811905	472.382924	11.361946
10.444612	455.720410	11.366963
10.961839	460.747147	11.371981
10.919219	464.172563	11.376999
10.593149	440.239114	11.382016
10.354910	446.246515	11.387034
10.692099	465.496407	11.392051
10.728683	464.399237	11.397069
11.053252	467.679444	11.402087
11.253123	456.047633	11.407104
10.805922	448.480399	11.412122
10.731539	440.854709	11.417139
10.697335	440.621423	11.422157
10.712546	445.109691	11.427175
10.596659	454.591816	11.432192
10.845970	462.476219	11.437210
10.763760	450.441022	11.442227
10.867745	455.845826	11.447245
10.674149	466.785282	11.452263
10.850497	458.892015	11.457280
11.096368	462.578845	11.462298
10.809426	463.740587	11.467315
11.142983	469.354158	11.472333
11.019896	462.945900	11.477351
11.063907	458.730140	11.482368
10.866448	468.026976	11.487386
10.925256	461.170538	11.492403
11.140233	459.827891	11.497421
10.524833	456.204760	11.502439
10.839337	453.520942	11.507456
10.704759	461.492696	11.512474
10.796949	464.192928	11.517491
10.956388	458.151481	11.522509
10.860737	465.522833	11.527527
11.115136	459.000730	11.532544
11.352077	463.299441	11.537562
10.818895	454.095181	11.542579
11.155288	455.570953	11.547597
10.749893	462.182931	11.552615
10.939359	457.381932	11.557632
10.733327	461.644418	11.562650
10.391806	449.797812	11.567667
10.799148	462.127706	11.572685
10.985301	475.905091	11.577703
11.330101	474.533412	11.582720
11.500605	483.151959	11.587738
11.385569	466.140330	11.592755
11.326849	459.186804	11.597773
11.099253	460.870025	11.602791
11.438977	457.778382	11.607808
11.345514	445.086525	11.612826
11.356854	457.194810	11.617843
11.619646	455.023861	11.622861
10.845473	472.163210	11.627879
10.734745	454.367088	11.632896
10.833463	462.010192	11.637914
10.938128	453.941804	11.642931
11.224119	467.982743	11.647949
11.657242	483.842898	11.652967
11.717815	475.111058	11.657984
11.096327	460.451458	11.663002
11.150175	457.600619	11.668019
11.328360	447.083879	11.673037
11.031022	464.953210	11.678055
11.718101	471.830823	11.683072
11.600617	460.761780	11.688090
11.270330	469.693640	11.693107
11.408453	456.392951	11.698125
11.491061	457.021379	11.703143
11.393431	446.656398	11.708160
11.481541	446.923952	11.713178
10.785997	456.264811	11.718195
11.354725	454.721314	11.723213
11.565950	480.436860	11.728231
11.587266	475.038674	11.733248
11.746453	466.668121	11.738266
11.430731	452.735299	11.743283
11.295029	447.096393	11.748301
11.173240	460.735126	11.753319
11.527703	468.808117	11.758336
11.799017	481.160998	11.763354
11.468333	466.130273	11.768371
11.574120	454.290534	11.773389
11.270470	465.133436	11.778407
11.530660	470.892077	11.783424
11.718024	475.817360	11.788442
11.641359	471.969006	11.793459
11.619688	466.303377	11.798477
11.319354	467.176940	11.803495
11.795554	461.154882	11.808512
11.931386	468.552733	11.813530
11.487352	460.332940	11.818547
11.567777	451.030627	11.823565
11.564592	448.460714	11.828583
11.560532	453.436319	11.833600
11.557915	464.999688	11.838618
11.727083	478.991060	11.843635
11.828354	483.883141	11.848653
11.956220	467.462047	11.853671
11.759712	461.119652	11.858688
11.811070	458.055292	11.863706
11.485180	448.680884	11.868723
11.512980	456.108291	11.873741
11.576653	472.666461	11.878759
11.752030	476.613219	11.883776
12.094777	481.224008	11.888794
11.608866	482.699577	11.893811
12.125239	476.583688	11.898829
11.691705	479.252026	11.903847
11.522787	471.462551	11.908864
11.604027	480.386339	11.913882
11.628975	480.968500	11.918899
11.814055	471.808100	11.923917
11.668895	484.168993	11.928935
11.963559	475.818853	11.933952
12.072068	488.726291	11.938970
11.536780	495.789089	11.943987
12.178975	478.160287	11.949005
11.684318	487.783257	11.954023
11.635192	483.201759	11.959040
11.853687	485.460737	11.964058
11.794097	493.543220	11.969075
11.636007	477.482889	11.974093
11.313624	476.674126	11.979111
11.750360	496.949812	11.984128
12.193811	508.488308	11.989146
12.146726	505.120687	11.994163
12.419971	494.769861	11.999181
12.075292	487.383854	12.004199
12.085030	480.865369	12.009216
12.318994	471.810745	12.014234
12.045870	478.670402	12.019251
12.164544	474.739580	12.024269
12.309689	470.898853	12.029287
12.190229	474.466076	12.034304
12.090129	466.725750	12.039322
11.744253	464.822278	12.044339
12.242829	474.027516	12.049357
12.019930	470.188174	12.054375
11.906748	470.623905	12.059392
12.155086	466.109275	12.064410
12.001114	470.287586	12.069427
12.237226	476.481713	12.074445
12.162389	468.745772	12.079463
11.927478	474.172932	12.084480
12.694715	484.658505	12.089498
12.152672	484.249253	12.094515
12.432750	465.459200	12.099533
12.348136	477.481509	12.104551
12.279740	476.255556	12.109568
12.345739	464.246633	12.114586
11.897518	478.640361	12.119603
12.085947	466.958868	12.124621
12.008284	493.970146	12.129639
12.114506	496.464662	12.134656
12.208613	509.659479	12.139674
12.235382	506.367036	12.144691
12.502700	499.255205	12.149709
12.644214	510.964441	12.154727
12.858495	499.990906	12.159744
12.501472	490.889376	12.164762
12.310919	480.628982	12.169779
12.257603	491.167399	12.174797
12.626353	487.965562	12.179815
12.212724	484.558440	12.184832
12.332652	487.341771	12.189850
12.763004	505.809055	12.194867
12.427331	504.077380	12.199885
12.448928	514.043706	12.204903
12.722754	503.133740	12.209920
12.646614	487.959966	12.214938
12.190255	482.141802	12.219955
12.582944	479.514434	12.224973
12.682824	494.650304	12.229991
12.389104	503.684287	12.235008
12.858599	488.844962	12.240026
12.468147	498.331648	12.245043
12.485243	490.394026	12.250061
12.540182	498.173687	12.255079
12.527916	502.981900	12.260096
12.851480	503.643528	12.265114
12.859776	511.431592	12.270131
12.770338	494.395037	12.275149
12.437305	493.289373	12.280167
12.358116	483.373884	12.285184
12.495992	496.925653	12.290202
12.799724	500.678998	12.295219
12.926700	493.262082	12.300237
12.824281	506.740404	12.305255
12.583067	505.286072	12.310272
13.223125	502.865999	12.315290
12.782713	496.490977	12.320307
12.520822	490.157406	12.325325
12.720413	489.159354	12.330343
12.614289	502.348285	12.335360
12.705607	504.934913	12.340378
12.777625	513.954024	12.345395
12.560489	509.835332	12.350413
12.605257	508.939619	12.355431
12.379949	504.761563	12.360448
12.841287	501.802243	12.365466
12.519134	506.382886	12.370483
12.538366	510.201748	12.375501
12.982874	508.976645	12.380519
12.510830	507.303326	12.385536
12.785713	510.742116	12.390554
13.030387	528.369226	12.395571
13.122780	516.726100	12.400589
13.049354	501.747001	12.405607
12.859753	502.803210	12.410624
13.024288	509.142321	12.415642
12.741321	515.600357	12.420659
13.379471	512.881545	12.425677
13.048669	509.030798	12.430695
12.943631	506.696854	12.435712
13.153059	498.771038	12.440730
13.147872	508.963592	12.445747
13.175283	497.520944	12.450765
12.990185	497.655830	12.455783
12.769869	502.820503	12.460800
13.314999	498.918296	12.465818
13.662760	498.648851	12.470835
13.217897	510.980077	12.475853
13.388560	500.696288	12.480871
12.934649	503.130152	12.485888
13.286346	501.362136	12.490906
13.047934	486.411891	12.495923
12.711567	500.723192	12.500941
13.369421	491.118192	12.505959
13.294545	493.330692	12.510976
13.492275	498.344309	12.515994
13.041473	494.311961	12.521011
12.939742	494.145530	12.526029
13.077657	499.982940	12.531047
13.448914	508.138494	12.536064
13.957814	502.347090	12.541082
13.297667	498.557364	12.546099
13.137710	497.126703	12.551117
13.195752	483.297801	12.556135
13.037967	490.699508	12.561152
13.447003	491.859700	12.566170
13.193227	501.302547	12.571187
13.379863	514.032956	12.576205
13.633686	509.504811	12.581223
13.345503	501.374965	12.586240
13.334144	501.618907	12.591258
13.311817	497.744444	12.596275
13.545074	510.819338	12.601293
13.626256	517.597533	12.606311
13.445330	513.166029	12.611328
13.478534	503.154312	12.616346
13.450200	499.448819	12.621363
13.375578	504.944068	12.626381
13.602443	503.138228	12.631399
13.339499	516.742377	12.636416
13.540657	512.894056	12.641434
13.472113	516.836359	12.646451
13.593557	520.673758	12.651469
14.049991	514.462466	12.656487
13.560139	522.857750	12.661504
13.720781	505.108733	12.666522
13.169573	506.617039	12.671539
13.652746	512.210035	12.676557
13.590486	507.747507	12.681575
13.716670	526.255929	12.686592
13.799006	519.801990	12.691610
13.682126	526.318000	12.696627
13.588399	516.256792	12.701645
13.776528	518.111920	12.706663
13.723995	523.795514	12.711680
13.957593	522.318118	12.716698
13.710187	526.416235	12.721715
13.425268	524.345333	12.726733
13.743878	520.551405	12.731751
13.763732	523.589028	12.736768
13.483433	522.654138	12.741786
13.499854	524.033710	12.746803
13.561607	523.245010	12.751821
13.882026	517.030117	12.756839
13.642028	514.688657	12.761856
13.697036	516.940904	12.766874
13.856848	515.921674	12.771891
13.529884	516.144163	12.776909
13.913397	513.228503	12.781927
13.877407	516.817073	12.786944
14.042430	518.110879	12.791962
13.580465	518.389234	12.796979
13.267776	531.278338	12.801997
14.065121	534.119187	12.807015
14.173725	546.884364	12.812032
14.222942	551.051949	12.817050
14.525137	544.375879	12.822067
14.204866	537.965831	12.827085
13.929723	511.352350	12.832103
13.812205	519.632275	12.837120
14.179954	520.025237	12.842138
14.126675	524.127486	12.847155
13.918671	515.899164	12.852173
14.234199	512.150620	12.857191
14.189893	525.627031	12.862208
14.023314	519.713927	12.867226
14.286292	518.383319	12.872243
14.259777	519.579276	12.877261
14.116290	513.929528	12.882279
13.831927	516.439096	12.887296
14.318979	526.524929	12.892314
14.511028	526.110679	12.897331
14.162426	519.080252	12.902349
14.441085	514.248751	12.907367
14.006378	513.421941	12.912384
14.122722	519.882776	12.917402
14.314829	528.951624	12.922419
14.398867	524.864145	12.927437
14.074903	514.158743	12.932455
14.506130	530.191371	12.937472
14.280587	534.499514	12.942490
14.480982	527.341949	12.947507
14.434754	532.883589	12.952525
14.375578	510.348545	12.957543
14.095151	525.876556	12.962560
14.663319	543.540069	12.967578
14.841604	525.379731	12.972595
14.288601	524.656605	12.977613
14.464442	507.008793	12.982631
14.253935	522.191652	12.987648
14.231712	519.436919	12.992666
14.594159	530.256980	12.997683
14.268711	541.260494	13.002701
15.062240	540.637323	13.007719
14.477848	525.264981	13.012736
14.415569	526.732149	13.017754
14.552711	513.007644	13.022771
14.498020	523.874985	13.027789
14.495966	523.417827	13.032807
14.526103	532.888760	13.037824
14.569243	549.933084	13.042842
15.195635	546.216117	13.047859
14.527859	536.910354	13.052877
14.512569	517.906502	13.057895
14.616355	524.255068	13.062912
14.462058	542.959633	13.067930
14.893941	539.016300	13.072947
14.786603	556.435525	13.077965
14.639020	549.654387	13.082983
14.460695	548.617819	13.088000
14.776636	548.392305	13.093018
15.017601	544.845013	13.098035
14.766973	547.442496	13.103053
14.937586	543.458004	13.108071
14.730793	534.829651	13.113088
14.650473	537.312686	13.118106
14.778031	548.477616	13.123123
14.781394	546.353364	13.128141
14.855556	536.493388	13.133159
14.964088	542.828975	13.138176
14.644914	544.485812	13.143194
14.884981	536.556980	13.148211
14.955098	555.954839	13.153229
14.749145	535.845202	13.158247
14.952773	539.102408	13.163264
14.947797	541.478425	13.168282
14.961695	537.748526	13.173299
14.773517	548.289884	13.178317
14.858885	536.604015	13.183335
14.873237	550.530208	13.188352
14.938602	548.576185	13.193370
15.386640	531.322940	13.198387
15.147266	554.034270	13.203405
14.503150	542.378414	13.208423
14.807796	546.504969	13.213440
14.988738	547.129156	13.218458
15.017343	543.926343	13.223475
14.926930	541.284232	13.228493
14.957680	536.108337	13.233511
15.029602	534.586609	13.238528
14.860797	543.688735	13.243546
15.184866	549.014494	13.248563
15.383001	560.277394	13.253581
15.500522	552.991808	13.258599
15.175786	546.165650	13.263616
15.244295	538.970241	13.268634
15.297463	538.586716	13.273651
15.153086	543.696933	13.278669
15.052411	530.283509	13.283687
15.467803	541.280420	13.288704
15.158279	550.805133	13.293722
15.646021	548.207017	13.298739
15.337834	547.889406	13.303757
15.291867	536.287040	13.308775
15.349329	540.404550	13.313792
15.571060	551.646224	13.318810
15.643905	545.058240	13.323827
15.168377	532.701144	13.328845
15.391814	531.466913	13.333863
15.441164	534.318302	13.338880
15.467028	541.647961	13.343898
15.095553	542.153833	13.348915
15.297341	560.641930	13.353933
15.458374	561.602510	13.358951
15.510314	573.289497	13.363968
15.699167	560.013597	13.368986
15.741316	563.247503	13.374003
15.689504	554.918364	13.379021
15.798612	560.381106	13.384039
15.699589	541.593974	13.389056
15.465481	536.385288	13.394074
15.448846	549.568524	13.399091
15.494939	560.065961	13.404109
15.537964	563.246976	13.409127
15.702111	559.330760	13.414144
15.585668	565.184150	13.419162
15.699035	565.149659	13.424179
15.872800	555.434498	13.429197
15.655010	559.957072	13.434215
15.932899	558.848951	13.439232
16.067622	561.232392	13.444250
15.814972	547.907931	13.449267
15.481498	549.215726	13.454285
15.474007	555.403301	13.459303
15.905070	559.725755	13.464320
15.690473	562.441080	13.469338
16.136521	553.468954	13.474355
15.834370	553.097502	13.479373
15.772207	550.081898	13.484391
15.857543	555.674231	13.489408
15.667595	564.588071	13.494426
16.209125	556.262925	13.499443
15.883091	556.027972	13.504461
15.732858	562.192592	13.509479
16.287724	550.570930	13.514496
15.829906	561.783500	13.519514
16.179845	553.118144	13.524531
16.110889	555.610227	13.529549
15.611232	553.649693	13.534567
15.791722	546.346128	13.539584
15.616936	559.565939	13.544602
15.869859	555.608877	13.549619
15.735465	557.234688	13.554637
15.842470	554.558769	13.559655
16.047608	551.702692	13.564672
15.710970	561.951530	13.569690
15.920719	569.174846	13.574707
16.651739	573.947537	13.579725
16.450218	574.874348	13.584743
16.233056	553.879710	13.589760
16.042466	554.195782	13.594778
16.127103	553.667911	13.599795
16.178846	550.659954	13.604813
16.164042	571.914802	13.609831
16.367926	558.675387	13.614848
16.277535	577.055520	13.619866
16.509521	578.025434	13.624883
16.308346	562.955105	13.629901
16.352905	562.058932	13.634919
16.242715	541.847161	13.639936
16.398306	557.593839	13.644954
16.573841	562.105834	13.649971
16.432692	560.886189	13.654989
16.028905	546.541739	13.660007
16.563255	559.464872	13.665024
16.657911	571.194001	13.670042
16.511471	550.555815	13.675059
16.415455	553.530915	13.680077
16.068004	547.301992	13.685095
16.656785	571.388884	13.690112
16.563384	579.335296	13.695130
16.787754	567.757805	13.700147
16.919567	559.237917	13.705165
16.461755	556.721169	13.710183
16.849926	542.290624	13.715200
16.467959	551.190725	13.720218
16.366292	555.231800	13.725235
16.244961	549.347814	13.730253
16.351301	577.668227	13.735271
16.667615	569.385705	13.740288
16.860322	591.107958	13.745306
16.444451	581.830308	13.750323
16.909090	585.690128	13.755341
16.927549	582.706461	13.760359
16.871763	571.623796	13.765376
16.805044	583.805797	13.770394
16.888240	590.246948	13.775411
16.767969	588.339046	13.780429
16.516415	587.869191	13.785447
16.858597	587.927865	13.790464
16.735380	586.017597	13.795482
16.586327	588.479722	13.800499
17.098100	577.231524	13.805517
16.735145	583.644551	13.810535
16.819214	577.438579	13.815552
16.754829	584.968568	13.820570
16.871353	583.980695	13.825587
17.290193	583.219284	13.830605
16.732445	583.773160	13.835623
17.197929	573.911276	13.840640
16.947051	581.508689	13.845658
16.821198	576.414259	13.850675
16.821760	575.981761	13.855693
16.943611	578.727987	13.860711
17.041903	580.002714	13.865728
16.988686	581.935619	13.870746
16.997092	579.189787	13.875763
17.266146	574.083926	13.880781
16.685889	591.036275	13.885799
17.032465	575.824048	13.890816
17.002023	579.139919	13.895834
16.948087	579.769858	13.900851
17.172559	581.278210	13.905869
16.985591	579.455332	13.910887
17.402929	581.766881	13.915904
17.436981	579.882189	13.920922
16.952259	583.044044	13.925939
17.273288	575.435604	13.930957
17.087640	582.299450	13.935975
17.372175	584.682543	13.940992
17.464187	600.258312	13.946010
17.251537	601.776119	13.951027
17.368912	584.026091	13.956045
17.450676	589.927134	13.961063
17.205880	596.921209	13.966080
17.102400	607.059023	13.971098
17.344269	601.031451	13.976115
17.642701	600.384407	13.981133
17.258726	605.306824	13.986151
17.432146	600.900972	13.991168
17.531867	601.765310	13.996186
17.717219	598.103894	14.001203
17.535205	594.835011	14.006221
17.610679	594.633588	14.011239
17.856708	593.469816	14.016256
17.823728	591.059988	14.021274
17.581156	596.758875	14.026291
17.680950	586.346906	14.031309
17.389001	592.845230	14.036327
17.768076	594.272829	14.041344
18.022609	592.984842	14.046362
17.555504	588.593128	14.051379
17.679292	576.919774	14.056397
17.435645	587.279024	14.061415
17.792175	585.060290	14.066432
17.686074	589.438358	14.071450
17.683802	598.245530	14.076467
18.165676	591.148978	14.081485
17.581149	600.689054	14.086503
17.627267	591.050465	14.091520
17.545764	590.220389	14.096538
17.430967	595.332231	14.101555
17.791807	593.124297	14.106573
17.812032	604.372346	14.111591
17.825455	593.227352	14.116608
17.839228	602.927366	14.121626
17.733653	597.256365	14.126643
17.893917	592.047338	14.131661
18.013194	602.044323	14.136679
17.789840	595.053977	14.141696
18.061308	592.034303	14.146714
17.675507	599.882126	14.151731
17.932019	586.502718	14.156749
17.805143	603.854276	14.161767
17.850919	599.040568	14.166784
17.954079	608.413376	14.171802
18.179192	625.063415	14.176819
18.612456	606.599971	14.181837
18.163986	596.461631	14.186855
18.296199	591.644958	14.191872
18.027732	590.477840	14.196890
18.232508	591.521923	14.201907
18.353085	588.383907	14.206925
18.167519	593.207994	14.211943
18.028038	584.035328	14.216960
18.363587	585.693795	14.221978
18.244832	576.224558	14.226995
18.160610	588.285956	14.232013
18.158140	584.951093	14.237031
18.036530	586.826910	14.242048
18.448476	602.735069	14.247066
18.529077	619.969404	14.252083
18.530092	614.384600	14.257101
18.248866	604.793307	14.262119
18.409554	604.366525	14.267136
18.670974	604.609083	14.272154
18.608049	603.864501	14.277171
18.659917	583.121566	14.282189
18.316806	588.973061	14.287207
18.279714	580.831102	14.292224
18.423359	583.735212	14.297242
18.541557	603.820913	14.302259
18.136044	603.409957	14.307277
18.615936	603.945087	14.312295
18.519480	614.284460	14.317312
18.663184	612.952790	14.322330
18.610118	620.399644	14.327347
18.786432	607.144177	14.332365
18.638170	621.644836	14.337383
18.680143	611.108278	14.342400
18.868503	602.573413	14.347418
18.679018	612.536503	14.352435
19.207616	607.069399	14.357453
18.592815	614.939524	14.362471
18.748700	604.882866	14.367488
19.075123	613.352124	14.372506
18.812735	605.843819	14.377523
19.171630	605.788534	14.382541
18.739856	589.493839	14.387559
18.606805	587.169038	14.392576
18.971667	590.674556	14.397594
18.445443	605.826518	14.402611
18.700358	598.697108	14.407629
19.013508	611.166484	14.412647
18.674026	610.881302	14.417664
18.862163	613.050945	14.422682
19.204436	614.573685	14.427699
18.853844	612.617441	14.432717
18.796205	614.071845	14.437735
18.891481	602.849551	14.442752
18.838450	604.979141	14.447770
18.817690	609.735358	14.452787
19.157970	604.866682	14.457805
18.803217	606.822260	14.462823
19.034453	612.760115	14.467840
19.164044	604.579676	14.472858
18.794553	612.275824	14.477875
19.175140	618.276680	14.482893
19.323750	627.536892	14.487911
19.134647	636.761301	14.492928
19.316807	628.528175	14.497946
19.292810	635.956160	14.502963
19.537057	617.875542	14.507981
19.234008	616.143482	14.512999
18.941507	611.351131	14.518016
19.560728	620.594875	14.523034
19.453510	622.516635	14.528051
19.158071	619.143483	14.533069
19.272486	629.012180	14.538087
19.444759	628.580039	14.543104
19.794876	631.617918	14.548122
19.337381	623.507031	14.553139
19.806529	613.526035	14.558157
19.293588	603.444300	14.563175
19.174189	614.091341	14.568192
19.679733	614.843153	14.573210
19.301124	637.949787	14.578227
19.595915	634.528888	14.583245
19.523394	629.021277	14.588263
19.245186	637.506525	14.593280
19.579609	633.217534	14.598298
19.170824	633.452955	14.603315
19.690542	627.723878	14.608333
19.765008	630.487589	14.613351
19.464740	639.057176	14.618368
19.739311	631.658019	14.623386
19.606340	634.315683	14.628403
19.542335	637.119400	14.633421
19.480645	639.288017	14.638439
19.521323	631.830680	14.643456
19.637008	640.092995	14.648474
19.431450	647.291689	14.653491
19.837659	651.161280	14.658509
20.065787	653.196983	14.663527
20.177730	658.037465	14.668544
20.147136	645.152411	14.673562
20.070471	633.960082	14.678579
19.735977	628.028335	14.683597
19.991766	618.939414	14.688615
19.852299	618.039305	14.693632
20.475173	630.208449	14.698650
19.943222	624.201087	14.703667
19.722384	624.401710	14.708685
19.938011	620.175062	14.713703
20.160882	632.250695	14.718720
20.183624	622.778515	14.723738
20.248550	633.615145	14.728755
20.081729	627.740221	14.733773
19.969498	622.421520	14.738791
19.750401	639.125792	14.743808
20.234238	637.517582	14.748826
20.495477	646.651340	14.753843
20.385247	651.381418	14.758861
20.238951	660.188709	14.763879
19.746134	658.536518	14.768896
20.506042	649.710267	14.773914
20.770004	656.315237	14.778931
20.975099	635.506169	14.783949
20.216337	628.278661	14.788967
20.181900	620.738190	14.793984
20.333093	623.852633	14.799002
20.260270	623.746863	14.804019
20.281054	622.505078	14.809037
20.731926	622.034968	14.814055
20.294287	628.179603	14.819072
20.399665	623.985540	14.824090
20.572537	631.739089	14.829107
20.389497	638.953838	14.834125
20.431390	625.669200	14.839143
20.410651	650.811085	14.844160
20.666047	639.448645	14.849178
20.755616	645.807878	14.854195
20.792549	649.608104	14.859213
21.041565	625.101963	14.864231
20.567509	627.083557	14.869248
20.590744	611.440472	14.874266
20.435685	626.187486	14.879283
20.657557	632.757579	14.884301
20.720322	627.568097	14.889319
20.742446	644.075161	14.894336
20.650966	645.757755	14.899354
20.721347	643.863804	14.904371
20.717434	651.807864	14.909389
20.984862	638.485355	14.914407
20.783759	652.010815	14.919424
20.910148	640.707087	14.924442
20.700538	636.495894	14.929459
20.710312	645.395473	14.934477
20.984620	651.159132	14.939495
20.814002	649.921421	14.944512
20.621712	635.098716	14.949530
20.610864	651.476224	14.954547
20.623765	643.036461	14.959565
21.046914	649.318428	14.964583
20.665326	651.091573	14.969600
20.936892	658.459607	14.974618
21.293279	665.879658	14.979635
21.342628	659.960930	14.984653
21.257743	644.950322	14.989671
21.051069	637.884478	14.994688
21.215688	638.524848	14.999706
21.118634	643.867291	15.004723
21.157833	646.308353	15.009741
21.505246	637.815773	15.014759
21.338389	636.460339	15.019776
21.555501	637.165839	15.024794
21.177005	636.485016	15.029811
21.188076	641.985245	15.034829
21.574653	635.886019	15.039847
21.233424	641.909630	15.044864
21.498288	638.854629	15.049882
21.507704	640.958258	15.054899
21.393415	637.160460	15.059917
21.399992	627.455464	15.064935
21.272959	641.213311	15.069952
21.171691	635.074352	15.074970
21.583338	649.692609	15.079987
21.479996	669.666906	15.085005
21.914688	660.696005	15.090023
21.609553	657.811359	15.095040
21.623505	649.692910	15.100058
21.479040	645.994961	15.105075
21.845537	654.369546	15.110093
21.912749	636.380157	15.115111
21.659943	642.742532	15.120128
21.472289	629.668231	15.125146
21.393325	640.461827	15.130163
21.454618	652.814915	15.135181
21.698496	659.703269	15.140199
22.170582	661.392518	15.145216
22.029856	666.863225	15.150234
22.048481	652.303130	15.155251
21.584275	652.436216	15.160269
21.952163	642.113639	15.165287
21.458151	659.811997	15.170304
21.794431	652.237507	15.175322
21.964747	658.761811	15.180339
21.824575	660.363494	15.185357
21.794831	660.227283	15.190375
22.165936	666.407250	15.195392
22.215395	662.555719	15.200410
22.302038	665.373121	15.205427
22.299730	667.216636	15.210445
22.242330	653.311400	15.215463
22.019750	635.251027	15.220480
22.027754	653.692634	15.225498
22.158620	637.839648	15.230515
21.943831	655.349564	15.235533
22.188326	652.531837	15.240551
21.936417	649.876343	15.245568
22.023454	655.605511	15.250586
22.289013	658.518321	15.255603
22.098003	658.664025	15.260621
22.094244	655.527255	15.265639
22.250901	662.489953	15.270656
22.088365	652.831977	15.275674
22.466440	653.076809	15.280691
22.256272	656.726570	15.285709
22.323843	661.483557	15.290727
22.190618	663.245576	15.295744
21.912204	658.318822	15.300762
22.337294	656.080383	15.305779
22.264852	667.359636	15.310797
22.864250	674.593695	15.315815
22.529376	671.942658	15.320832
22.687102	659.578430	15.325850
22.601113	655.174002	15.330867
22.670422	654.904418	15.335885
22.475948	654.874548	15.340903
22.661841	662.524110	15.345920
22.606325	667.300061	15.350938
22.387983	660.842415	15.355955
22.419333	682.673140	15.360973
22.707725	694.380485	15.365991
22.681186	684.283560	15.371008
22.926741	688.155108	15.376026
23.277418	673.765176	15.381043
22.889484	695.037179	15.386061
22.971417	674.045596	15.391079
22.654488	670.044610	15.396096
22.862071	677.054105	15.401114
23.247061	680.384796	15.406131
22.797245	675.937159	15.411149
22.972154	674.867992	15.416167
23.084872	682.523851	15.421184
22.919204	669.315298	15.426202
23.102143	669.479210	15.431219
23.025064	665.450497	15.436237
23.180911	675.397007	15.441255
23.100420	666.329776	15.446272
22.651774	671.276874	15.451290
23.047736	670.423885	15.456307
23.180801	683.941976	15.461325
23.419793	686.113165	15.466343
22.995961	688.237028	15.471360
22.982891	689.636347	15.476378
23.063298	685.314136	15.481395
22.924847	689.570733	15.486413
22.844352	677.000630	15.491431
22.843800	697.237942	15.496448
22.936443	686.340566	15.501466
23.101350	689.577141	15.506483
23.110013	705.584920	15.511501
23.463652	708.082474	15.516519
23.632626	703.403562	15.521536
23.504487	712.294776	15.526554
23.995427	709.350699	15.531571
23.671085	688.823894	15.536589
23.373427	681.783890	15.541607
23.503044	688.402809	15.546624
23.130404	677.408936	15.551642
23.511347	682.883090	15.556659
23.516092	697.489121	15.561677
23.322384	695.339552	15.566695
23.423349	697.673879	15.571712
23.216256	711.339527	15.576730
23.402565	700.333865	15.581747
23.534298	706.777772	15.586765
23.702003	704.660191	15.591783
23.893201	702.200704	15.596800
23.690156	703.986960	15.601818
23.911258	699.926676	15.606835
23.772618	710.689737	15.611853
23.487999	695.857629	15.616871
23.538024	697.848277	15.621888
23.324807	702.926132	15.626906
24.075277	721.343730	15.631923
24.078468	722.192733	15.636941
24.513671	729.206657	15.641959
24.360154	711.463459	15.646976
24.042345	705.602434	15.651994
24.049502	699.645297	15.657011
24.108315	698.210545	15.662029
23.909170	699.352678	15.667047
24.427843	693.953017	15.672064
23.824461	698.531971	15.677082
24.294887	692.853232	15.682099
24.232992	699.637144	15.687117
24.202108	690.860168	15.692135
24.301232	700.769521	15.697152
23.957593	700.706044	15.702170
24.343075	699.785605	15.707187
24.243855	705.854764	15.712205
24.247908	701.249258	15.717223
24.377452	701.280486	15.722240
24.026851	697.248549	15.727258
24.295876	710.069031	15.732275
24.458028	715.886183	15.737293
24.595081	730.700652	15.742311
24.988803	725.433517	15.747328
24.469182	701.680531	15.752346
24.248481	698.793537	15.757363
24.358431	699.001690	15.762381
24.488168	714.371872	15.767399
24.746538	717.495488	15.772416
24.642654	728.557091	15.777434
24.601966	717.883360	15.782451
24.458155	715.742567	15.787469
24.541979	724.588822	15.792487
24.783728	726.094825	15.797504
24.412060	733.564369	15.802522
25.031715	725.270801	15.807539
24.911581	730.963676	15.812557
24.826914	724.712313	15.817575
25.010019	723.351490	15.822592
24.973192	729.639240	15.827610
24.756509	695.300319	15.832627
24.811453	718.552119	15.837645
24.966398	720.295948	15.842663
25.271355	714.566804	15.847680
24.655016	717.238329	15.852698
24.943519	710.915071	15.857715
25.195089	715.089609	15.862733
24.973006	716.528686	15.867751
25.263159	699.093411	15.872768
24.553908	702.801252	15.877786
24.626034	706.878792	15.882803
24.550484	716.645499	15.887821
24.642358	722.385996	15.892839
24.977057	713.069158	15.897856
24.709628	724.670383	15.902874
25.132562	717.415337	15.907891
24.967943	733.878962	15.912909
25.270873	752.118928	15.917927
25.714475	742.264587	15.922944
25.584506	736.697153	15.927962
25.279829	729.759251	15.932979
25.562996	720.994619	15.937997
25.276909	720.346249	15.943015
25.319102	717.614293	15.948032
25.184367	718.790066	15.953050
25.260565	735.203565	15.958067
25.661823	741.171040	15.963085
25.409803	748.406686	15.968103
25.797027	742.936425	15.973120
25.928334	746.200412	15.978138
25.644229	740.314319	15.983155
25.464628	726.040112	15.988173
25.388976	744.732517	15.993191
25.989663	737.109274	15.998208
25.539659	747.293422	16.003226
25.499917	745.874854	16.008243
25.606586	736.857248	16.013261
25.552133	742.413115	16.018279
25.747351	753.327099	16.023296
25.236550	746.516935	16.028314
25.786525	735.330505	16.033331
25.848335	752.486712	16.038349
25.626713	755.619590	16.043367
25.976535	737.588006	16.048384
25.673441	741.171662	16.053402
25.688962	744.076901	16.058419
25.662709	760.504306	16.063437
25.889337	773.598430	16.068455
26.345082	777.091729	16.073472
26.455238	769.012427	16.078490
26.492091	763.524186	16.083507
26.481149	739.365981	16.088525
26.534804	752.608137	16.093543
26.644547	731.596627	16.098560
26.100112	745.592606	16.103578
26.169557	732.835997	16.108595
26.321107	734.302587	16.113613
26.096957	738.870252	16.118631
26.445490	738.108546	16.123648
26.078194	741.339396	16.128666
26.284946	727.919475	16.133683
26.267819	725.893940	16.138701
26.253122	727.205654	16.143719
26.694888	727.634218	16.148736
26.334221	745.705543	16.153754
26.024221	730.719358	16.158771
26.409788	728.081121	16.163789
26.083794	744.825609	16.168807
26.496254	746.905063	16.173824
26.506957	767.318330	16.178842
26.617510	769.326538	16.183859
26.868512	765.113391	16.188877
26.815292	770.236862	16.193895
26.639665	764.136612	16.198912
26.578577	780.223895	16.203930
26.549540	765.456452	16.208947
27.049914	764.663749	16.213965
26.878881	767.553372	16.218983
27.045128	755.046544	16.224000
26.890049	747.164796	16.229018
27.194253	735.404037	16.234035
27.008689	733.032194	16.239053
26.874108	734.132465	16.244071
26.732607	727.051971	16.249088
26.624256	723.823928	16.254106
26.612616	741.720173	16.259123
27.112872	751.793249	16.264141
26.976811	764.229031	16.269159
27.266319	756.709061	16.274176
27.167190	757.372946	16.279194
26.970479	760.565475	16.284211
27.345138	754.038726	16.289229
26.858165	762.484244	16.294247
27.326187	751.846875	16.299264
26.983929	760.848585	16.304282
26.950947	764.500778	16.309299
27.162598	748.444895	16.314317
27.079445	762.391231	16.319335
27.187385	759.583947	16.324352
27.088732	758.411682	16.329370
26.875383	764.480338	16.334387
27.179250	759.450439	16.339405
27.133265	772.594926	16.344423
27.086689	788.071568	16.349440
27.454663	777.475512	16.354458
27.320010	791.446721	16.359475
27.624516	785.928413	16.364493
27.461977	783.605011	16.369511
27.566796	779.944658	16.374528
27.237601	792.123554	16.379546
27.263240	792.461072	16.384563
27.664437	791.190459	16.389581
27.835421	792.085445	16.394599
27.866108	781.424379	16.399616
27.855663	782.514570	16.404634
27.574830	793.680447	16.409651
27.787272	794.454234	16.414669
27.676831	791.838022	16.419687
27.885271	792.932390	16.424704
28.268926	794.313789	16.429722
27.816489	804.505757	16.434739
27.602938	791.416900	16.439757
27.715004	797.194928	16.444775
28.323613	807.252300	16.449792
28.340256	816.114433	16.454810
27.883658	808.682306	16.459827
28.465695	801.572354	16.464845
28.321818	797.771631	16.469863
28.215180	783.810056	16.474880
28.184011	776.898575	16.479898
28.144480	784.251851	16.484915
28.273335	769.697539	16.489933
28.224095	782.509467	16.494951
28.282612	775.305068	16.499968
28.125851	774.435460	16.504986
28.131861	799.408436	16.510003
28.491854	801.388123	16.515021
28.520000	803.510231	16.520039
28.516793	810.862536	16.525056
28.563737	797.741844	16.530074
28.130887	793.410834	16.535091
28.555697	799.436929	16.540109
28.489701	814.505662	16.545127
28.633711	809.053526	16.550144
28.295462	810.540641	16.555162
28.442508	801.924321	16.560179
28.914334	804.353453	16.565197
28.699672	807.941208	16.570215
28.729467	806.447966	16.575232
28.816550	800.467741	16.580250
28.639142	805.835622	16.585267
28.721451	806.770750	16.590285
28.404798	806.324930	16.595303
28.803105	810.553872	16.600320
29.046534	795.964168	16.605338
28.941716	807.639451	16.610355
28.855522	803.221237	16.615373
28.733578	803.038757	16.620391
28.554125	807.198342	16.625408
29.047787	805.097343	16.630426
28.855963	809.495249	16.635443
28.902622	799.679897	16.640461
28.912721	805.216361	16.645479
28.899417	804.417319	16.650496
28.897151	795.667437	16.655514
28.697333	816.326838	16.660531
29.116528	825.437849	16.665549
29.119665	833.707156	16.670567
29.301251	828.591950	16.675584
29.294119	832.160571	16.680602
29.087642	841.850291	16.685619
29.297613	830.257563	16.690637
29.333664	836.992482	16.695655
29.427507	831.140436	16.700672
29.558034	823.945174	16.705690
29.311265	828.480193	16.710707
29.409171	824.128874	16.715725
29.422898	825.444757	16.720743
29.660467	826.754451	16.725760
29.795016	825.908931	16.730778
29.386676	827.187887	16.735795
29.560195	828.073994	16.740813
29.501898	819.672074	16.745831
29.436056	837.060751	16.750848
29.811556	835.170282	16.755866
29.683738	824.104553	16.760883
29.403846	830.013297	16.765901
29.620136	834.370929	16.770919
29.808290	849.294764	16.775936
30.322628	848.893575	16.780954
30.093536	849.615351	16.785971
29.875390	839.815293	16.790989
30.145460	827.297056	16.796007
29.908870	820.556681	16.801024
30.384107	821.491630	16.806042
29.969702	817.123221	16.811059
29.999103	817.662345	16.816077
30.270024	817.573378	16.821095
29.968987	823.134399	16.826112
29.768447	817.287214	16.831130
29.858834	835.815507	16.836147
30.105972	842.408479	16.841165
30.170569	843.539414	16.846183
30.522712	854.229051	16.851200
30.577217	842.096065	16.856218
30.100014	852.315677	16.861235
30.405055	841.529030	16.866253
30.507481	841.815875	16.871271
30.404369	847.873530	16.876288
30.655824	848.885218	16.881306
30.219568	846.516306	16.886323
30.484799	841.489321	16.891341
30.537932	844.038525	16.896359
30.377058	851.152288	16.901376
30.797319	844.616981	16.906394
30.460519	848.529204	16.911411
30.682363	840.485631	16.916429
30.485420	842.109408	16.921447
30.250675	852.512830	16.926464
30.530325	836.646368	16.931482
30.780876	851.469655	16.936499
30.682369	844.169246	16.941517
30.720784	843.015459	16.946535
30.534460	844.024011	16.951552
30.788813	850.056448	16.956570
30.473515	869.405915	16.961587
30.795843	879.965383	16.966605
30.978210	878.294291	16.971623
30.953569	869.947009	16.976640
31.154746	867.374350	16.981658
30.922778	876.282030	16.986675
31.192326	861.205751	16.991693
31.109454	872.331198	16.996711
30.869954	867.445573	17.001728
30.785284	863.746939	17.006746
30.946152	871.040670	17.011763
31.064590	879.929317	17.016781
31.237402	863.544360	17.021799
31.361569	871.091453	17.026816
31.282062	870.098659	17.031834
31.408013	884.513611	17.036851
31.489724	887.314156	17.041869
31.913518	878.460460	17.046887
31.268708	875.738578	17.051904
31.583135	858.390138	17.056922
31.338132	866.786477	17.061939
31.590277	873.931684	17.066957
31.763266	882.005756	17.071975
31.590714	885.914858	17.076992
31.675418	885.454866	17.082010
31.832168	895.959242	17.087027
31.625673	891.315060	17.092045
31.848605	903.320438	17.097063
32.085807	884.612535	17.102080
31.476008	873.988556	17.107098
31.898552	884.576636	17.112115
31.654029	889.213940	17.117133
32.061928	890.407320	17.122151
32.118599	891.424235	17.127168
32.003179	886.776616	17.132186
31.935204	895.590880	17.137203
32.268629	893.965875	17.142221
32.279915	884.304811	17.147239
32.179899	888.382504	17.152256
32.311598	874.946910	17.157274
32.120330	873.234431	17.162291
32.101318	868.639870	17.167309
32.121280	874.867616	17.172327
32.041020	889.531669	17.177344
32.377365	879.335679	17.182362
32.368177	895.431335	17.187379
32.294616	889.576226	17.192397
32.410492	891.022649	17.197415
32.170913	898.059298	17.202432
32.225592	898.105850	17.207450
32.284948	892.343716	17.212467
32.032205	888.696468	17.217485
32.378362	877.991273	17.222503
32.058800	888.644322	17.227520
32.142811	892.266486	17.232538
32.169098	888.909781	17.237555
32.201731	905.769460	17.242573
32.459105	912.651763	17.247591
32.484835	913.170929	17.252608
32.395798	915.928449	17.257626
32.425531	914.210640	17.262643
32.459162	917.754536	17.267661
33.099114	917.036775	17.272679
33.021966	933.846332	17.277696
33.270422	921.220488	17.282714
33.027213	912.378095	17.287731
32.990591	907.504987	17.292749
32.867001	906.462301	17.297767
33.042624	902.888429	17.302784
33.093679	907.949546	17.307802
32.674907	902.370830	17.312819
32.754429	931.620475	17.317837
32.997645	941.290365	17.322855
33.204753	942.338517	17.327872
33.063856	938.643252	17.332890
33.211377	935.055024	17.337907
33.024771	940.953808	17.342925
33.320467	935.717955	17.347943
33.164577	939.902811	17.352960
32.898041	940.561598	17.357978
33.227379	940.506966	17.362995
33.297213	945.191239	17.368013
33.615286	961.726301	17.373031
33.731256	955.852739	17.378048
34.160460	959.389829	17.383066
33.931764	945.944448	17.388083
33.512249	934.788185	17.393101
33.865308	931.338600	17.398119
33.751213	929.626647	17.403136
33.577853	927.099240	17.408154
33.742411	927.849555	17.413171
33.699141	926.030836	17.418189
33.607205	921.693444	17.423207
33.653468	938.322010	17.428224
33.781927	949.418987	17.433242
33.899783	952.334022	17.438259
33.928210	968.228297	17.443277
34.339513	951.189966	17.448295
33.969149	962.873822	17.453312
34.062560	950.341674	17.458330
34.155256	952.452249	17.463347
34.166630	958.769031	17.468365
34.212458	950.692293	17.473383
33.842033	957.205215	17.478400
33.882073	947.846490	17.483418
34.365818	946.597159	17.488435
34.140656	954.916363	17.493453
34.613681	949.649332	17.498471
34.322226	957.112026	17.503488
34.364005	954.212804	17.508506
34.449593	953.373892	17.513523
34.452792	961.548589	17.518541
34.286021	948.239306	17.523559
34.641344	957.632754	17.528576
34.371088	949.725748	17.533594
34.162550	953.436815	17.538611
34.382549	971.486945	17.543629
34.591018	967.125484	17.548647
34.720432	990.975127	17.553664
34.643888	989.477592	17.558682
34.769759	980.090002	17.563699
34.906099	985.788414	17.568717
35.013267	987.348864	17.573735
34.947550	992.420153	17.578752
34.981249	978.791151	17.583770
34.715444	979.294137	17.588787
34.844974	976.326974	17.593805
34.905557	979.873812	17.598823
34.984091	981.746813	17.603840
34.745073	983.461303	17.608858
34.882421	988.428771	17.613875
34.849684	987.240970	17.618893
34.907875	986.117461	17.623911
34.873768	980.784151	17.628928
34.692054	980.063609	17.633946
35.018998	985.077684	17.638963
35.278999	1006.332203	17.643981
35.405094	1006.654701	17.648999
35.566453	1016.721367	17.654016
35.337450	1006.449652	17.659034
35.781195	1003.754618	17.664051
35.482754	1006.963320	17.669069
35.643745	1002.113815	17.674087
35.444423	1011.959027	17.679104
35.547087	1007.422159	17.684122
35.667565	1001.899447	17.689139
35.354537	1003.119957	17.694157
35.820056	1000.457244	17.699175
35.941384	1007.684555	17.704192
35.740534	1002.295932	17.709210
35.990194	996.306184	17.714227
35.779257	1008.755029	17.719245
35.766398	999.941634	17.724263
35.839846	1006.171125	17.729280
35.785136	1004.296620	17.734298
36.028941	1004.147283	17.739315
35.645253	1001.076965	17.744333
35.633249	1009.155694	17.749351
35.762493	1006.780497	17.754368
35.874440	1012.747177	17.759386
36.016721	1025.398546	17.764403
36.150462	1043.331246	17.769421
36.121576	1031.523256	17.774439
36.174340	1031.443277	17.779456
36.045290	1039.147533	17.784474
36.430470	1030.428653	17.789491
36.662860	1035.452367	17.794509
36.334835	1036.101538	17.799527
36.749549	1034.801709	17.804544
36.168802	1038.043586	17.809562
36.568650	1032.785668	17.814579
36.379415	1038.513988	17.819597
36.705117	1027.226637	17.824615
36.545024	1031.714523	17.829632
36.377269	1033.133924	17.834650
36.736305	1026.059048	17.839667
36.639917	1023.680295	17.844685
36.481680	1029.023042	17.849703
36.674535	1032.209509	17.854720
36.506361	1040.325871	17.859738
36.628938	1046.141226	17.864755
36.574951	1055.453283	17.869773
37.016852	1061.458748	17.874791
37.126537	1049.796910	17.879808
37.147553	1055.225774	17.884826
37.177736	1051.231882	17.889843
37.217901	1063.382037	17.894861
37.150768	1053.048213	17.899879
37.297115	1051.085960	17.904896
37.312899	1057.581256	17.909914
37.196319	1040.328044	17.914931
37.419983	1049.482424	17.919949
37.416115	1054.007285	17.924967
37.558186	1052.301797	17.929984
37.126610	1049.515320	17.935002
37.524568	1043.295865	17.940019
37.422765	1046.407623	17.945037
37.174601	1044.904198	17.950055
37.453789	1035.656466	17.955072
37.384511	1043.409695	17.960090
37.266743	1044.228615	17.965107
37.184721	1038.586819	17.970125
37.201330	1045.748199	17.975143
37.315266	1043.597044	17.980160
37.497190	1063.666914	17.985178
37.618828	1080.476257	17.990195
37.759966	1075.399045	17.995213
37.786383	1089.873150	18.000231
37.717818	1076.923448	18.005248
37.650358	1080.007888	18.010266
38.218070	1081.090833	18.015283
37.999311	1084.806080	18.020301
38.028852	1083.221529	18.025319
38.183876	1071.143984	18.030336
38.259347	1077.659932	18.035354
38.385261	1080.015290	18.040371
37.879266	1068.100317	18.045389
38.192568	1073.372441	18.050407
38.604692	1075.843269	18.055424
38.252770	1079.832249	18.060442
38.286386	1064.255480	18.065459
38.424728	1077.134966	18.070477
38.252801	1080.405734	18.075495
38.701497	1080.429591	18.080512
38.361819	1077.352771	18.085530
38.839613	1063.121656	18.090547
38.516664	1074.261926	18.095565
38.292831	1071.944180	18.100583
39.031659	1071.728589	18.105600
38.248012	1077.676389	18.110618
38.143045	1079.200950	18.115635
38.902020	1083.394283	18.120653
38.738774	1104.302020	18.125671
39.158779	1093.718013	18.130688
39.027392	1100.971580	18.135706
39.094957	1084.051411	18.140723
39.091194	1077.888486	18.145741
38.687397	1074.324905	18.150759
39.001163	1076.503771	18.155776
39.136486	1092.681838	18.160794
39.291634	1092.222402	18.165811
39.151852	1095.125915	18.170829
39.098296	1098.360397	18.175847
39.254610	1098.049366	18.180864
39.102971	1098.497176	18.185882
39.438986	1087.705829	18.190899
39.396747	1088.150519	18.195917
39.310198	1093.674127	18.200935
39.514310	1092.413425	18.205952
39.308474	1101.272927	18.210970
39.172775	1088.737785	18.215987
39.257985	1096.930592	18.221005
39.496811	1093.005738	18.226023
39.386352	1088.650890	18.231040
39.099903	1095.536443	18.236058
39.595342	1093.340739	18.241075
39.683282	1089.898617	18.246093
39.619796	1105.786573	18.251111
39.768577	1109.072254	18.256128
39.673732	1121.103055	18.261146
39.804150	1124.133745	18.266163
39.624912	1116.623060	18.271181
39.692364	1122.687081	18.276199
39.786500	1125.333082	18.281216
39.768487	1124.967210	18.286234
39.976324	1119.339287	18.291251
39.614937	1122.826185	18.296269
39.767961	1127.979955	18.301287
40.080377	1130.770960	18.306304
40.394413	1137.489597	18.311322
40.438311	1152.120885	18.316339
40.549063	1144.587458	18.321357
40.253477	1127.184821	18.326375
40.622523	1129.524808	18.331392
40.465161	1116.786368	18.336410
40.298445	1111.998559	18.341427
40.596924	1128.091641	18.346445
40.528137	1128.717462	18.351463
40.579835	1136.954995	18.356480
40.652202	1138.284537	18.361498
40.659197	1131.455945	18.366515
40.720807	1143.340457	18.371533
40.466299	1135.329490	18.376551
40.848709	1144.063468	18.381568
40.530663	1142.503087	18.386586
40.823532	1131.679870	18.391603
40.935053	1142.604518	18.396621
40.699959	1141.391395	18.401639
40.871529	1140.302378	18.406656
40.806887	1145.814905	18.411674
41.084069	1144.081766	18.416691
41.096512	1138.571150	18.421709
40.815888	1144.284104	18.426727
41.072505	1141.804289	18.431744
41.116301	1152.602167	18.436762
41.404781	1172.199723	18.441779
41.612342	1165.237793	18.446797
41.678651	1170.004200	18.451815
41.562286	1154.653863	18.456832
41.484312	1137.769887	18.461850
41.497184	1136.395729	18.466867
41.519459	1135.929120	18.471885
41.334747	1137.348971	18.476903
41.725149	1146.420747	18.481920
41.762791	1154.736978	18.486938
41.693604	1161.552806	18.491955
41.554953	1144.712506	18.496973
41.590912	1160.843295	18.501991
41.791971	1157.033309	18.507008
41.525744	1165.339139	18.512026
41.731881	1172.181314	18.517043
41.772336	1155.815457	18.522061
41.831564	1168.916523	18.527079
42.156295	1159.117186	18.532096
41.937222	1158.515093	18.537114
42.046702	1162.322944	18.542131
41.926644	1158.788623	18.547149
41.641666	1170.299791	18.552167
42.042918	1170.590896	18.557184
42.193205	1185.477622	18.562202
42.461325	1181.684497	18.567219
42.567593	1187.328810	18.572237
42.506058	1195.790762	18.577255
42.523975	1179.911400	18.582272
42.308993	1171.834049	18.587290
42.157924	1181.944383	18.592307
42.686676	1186.719994	18.597325
42.590002	1182.694481	18.602343
43.033941	1182.445940	18.607360
42.687314	1188.129469	18.612378
42.603222	1179.078669	18.617395
42.976025	1178.766108	18.622413
42.877366	1184.606856	18.627431
42.699456	1178.270339	18.632448
42.980031	1182.410493	18.637466
42.514092	1185.881026	18.642483
42.855696	1181.946251	18.647501
42.716668	1184.341863	18.652519
42.591923	1182.165574	18.657536
43.115474	1177.435306	18.662554
43.070591	1186.831161	18.667571
43.238474	1175.217476	18.672589
42.993676	1183.438686	18.677607
42.937301	1175.626415	18.682624
43.176019	1188.944649	18.687642
43.309730	1194.647608	18.692659
43.569259	1206.904517	18.697677
43.459481	1208.692837	18.702695
43.396412	1198.898905	18.707712
43.641169	1206.896929	18.712730
43.782892	1214.659267	18.717747
43.754820	1202.253271	18.722765
43.779881	1196.129623	18.727783
43.630661	1192.109248	18.732800
43.896145	1184.337078	18.737818
43.272956	1187.555886	18.742835
43.691308	1194.169528	18.747853
43.690748	1207.722367	18.752871
43.796463	1200.484580	18.757888
43.959961	1195.357775	18.762906
43.665966	1203.294062	18.767923
43.948211	1198.843388	18.772941
43.852119	1210.367854	18.777959
43.858549	1202.161000	18.782976
44.356792	1201.640732	18.787994
43.934286	1214.121358	18.793011
44.092948	1214.248253	18.798029
43.951663	1228.357350	18.803047
44.119673	1226.603666	18.808064
44.490505	1223.538519	18.813082
44.391763	1221.527783	18.818099
44.847570	1218.300193	18.823117
44.405921	1224.048445	18.828135
44.299808	1219.963271	18.833152
44.381932	1222.147766	18.838170
44.243759	1220.692081	18.843187
44.552232	1219.578664	18.848205
44.712593	1231.489242	18.853223
44.873366	1218.367095	18.858240
44.884788	1212.647796	18.863258
44.443753	1229.111573	18.868275
44.972236	1229.999470	18.873293
45.054876	1252.938497	18.878311
45.445017	1247.423097	18.883328
45.258871	1224.365549	18.888346
45.067785	1218.683648	18.893363
45.145392	1222.606409	18.898381
45.058063	1215.907129	18.903399
45.552629	1234.683040	18.908416
45.263977	1221.757775	18.913434
45.047632	1228.024222	18.918451
45.104245	1241.102164	18.923469
45.507561	1242.106006	18.928487
45.491775	1249.054955	18.933504
45.507486	1247.207360	18.938522
45.499196	1252.050480	18.943539
45.807988	1246.627644	18.948557
45.689325	1243.849648	18.953575
45.634255	1257.351114	18.958592
45.523014	1236.786292	18.963610
45.374915	1251.645041	18.968627
45.498640	1246.476177	18.973645
45.496695	1256.064554	18.978663
45.403030	1250.988099	18.983680
45.906614	1249.719623	18.988698
45.387969	1249.758867	18.993715
45.707555	1259.887525	18.998733
45.491552	1257.179737	19.003751
45.977637	1268.387014	19.008768
46.203437	1258.367778	19.013786
45.731103	1270.398880	19.018803
46.044110	1271.194651	19.023821
46.076435	1270.656703	19.028839
46.187262	1282.639079	19.033856
46.519845	1289.511584	19.038874
46.538913	1292.309172	19.043891
46.674474	1293.937686	19.048909
46.621818	1296.123600	19.053927
46.800511	1296.376694	19.058944
46.994381	1280.811800	19.063962
46.495153	1277.590465	19.068979
46.636684	1260.759831	19.073997
46.772411	1272.506428	19.079015
46.718279	1291.287660	19.084032
46.906629	1283.609474	19.089050
47.028648	1289.960758	19.094067
47.068914	1286.965969	19.099085
47.202464	1283.026382	19.104103
46.827965	1290.404058	19.109120
47.175171	1283.258589	19.114138
47.360453	1285.493949	19.119155
47.308352	1277.266614	19.124173
47.140008	1279.402362	19.129191
47.167690	1287.336709	19.134208
47.528913	1272.517081	19.139226
47.583147	1279.946129	19.144243
47.545955	1280.558469	19.149261
47.488446	1281.802219	19.154279
46.966060	1285.746400	19.159296
47.518316	1262.271939	19.164314
47.233329	1280.641770	19.169331
47.411007	1279.401364	19.174349
47.389714	1276.824561	19.179367
47.364205	1281.911444	19.184384
47.098685	1286.582351	19.189402
47.453287	1295.991971	19.194419
48.158483	1305.790247	19.199437
48.106538	1297.485722	19.204455
47.939837	1309.574994	19.209472
48.179730	1296.074999	19.214490
47.788630	1304.351743	19.219507
47.883072	1310.050410	19.224525
48.051344	1305.833073	19.229543
47.998619	1307.325406	19.234560
48.457889	1303.012943	19.239578
48.268860	1300.911030	19.244595
47.993588	1299.295540	19.249613
47.905337	1297.180517	19.254631
47.993026	1327.150618	19.259648
48.530564	1325.981234	19.264666
48.395634	1328.540536	19.269683
48.485237	1333.116165	19.274701
48.798167	1326.058022	19.279719
48.587769	1323.786041	19.284736
48.848870	1314.529125	19.289754
48.797414	1328.139095	19.294771
48.871026	1320.727450	19.299789
48.842617	1312.339512	19.304807
48.620215	1329.691536	19.309824
48.700561	1313.192758	19.314842
48.905835	1324.227221	19.319859
49.138070	1319.779463	19.324877
48.964372	1318.219616	19.329895
48.615456	1315.067514	19.334912
49.481217	1330.479951	19.339930
49.844045	1350.248099	19.344947
49.390520	1330.254597	19.349965
49.689020	1325.280413	19.354983
49.067996	1324.069444	19.360000
49.193432	1317.748283	19.365018
49.526398	1324.208205	19.370035
49.642670	1341.663898	19.375053
49.566410	1345.312162	19.380071
49.449991	1342.797714	19.385088
49.566411	1342.639705	19.390106
49.595726	1346.504543	19.395123
49.674740	1339.523231	19.400141
49.765286	1338.842806	19.405159
49.745298	1350.082597	19.410176
50.141992	1339.440079	19.415194
49.951292	1346.567363	19.420211
49.950738	1344.954693	19.425229
50.200175	1341.088053	19.430247
49.618929	1339.115308	19.435264
49.949109	1330.971207	19.440282
50.024777	1360.968947	19.445299
50.264299	1370.531075	19.450317
50.515765	1366.622761	19.455335
50.299253	1376.483052	19.460352
50.794217	1371.386835	19.465370
50.730948	1365.400926	19.470387
50.518920	1366.232880	19.475405
50.741109	1363.447546	19.480423
50.469418	1370.758868	19.485440
50.865162	1359.643335	19.490458
50.631569	1360.442834	19.495475
50.542248	1361.384019	19.500493
50.966468	1358.336791	19.505511
50.645461	1361.233691	19.510528
50.803842	1357.009316	19.515546
51.177683	1360.255301	19.520563
50.750084	1366.548250	19.525581
51.088442	1359.098939	19.530599
50.751892	1362.254275	19.535616
50.860448	1368.747166	19.540634
50.761801	1374.562988	19.545651
50.957565	1390.438117	19.550669
51.367011	1388.718327	19.555687
50.960186	1391.134999	19.560704
51.345298	1389.908527	19.565722
51.593029	1390.864282	19.570739
51.255934	1391.491740	19.575757
51.502287	1384.005661	19.580775
51.460516	1397.457028	19.585792
51.855865	1405.610953	19.590810
51.975052	1404.293601	19.595827
52.035433	1415.016690	19.600845
52.172911	1383.273024	19.605863
51.714537	1388.806416	19.610880
52.286057	1378.445369	19.615898
52.295857	1371.833891	19.620915
52.148865	1382.296190	19.625933
52.179005	1374.382132	19.630951
52.140169	1375.249827	19.635968
52.196421	1380.262611	19.640986
51.986767	1381.962942	19.646003
52.166700	1386.886796	19.651021
52.274633	1379.007709	19.656039
51.888825	1402.706159	19.661056
52.129795	1414.864348	19.666074
52.859725	1413.221695	19.671091
52.635843	1412.387546	19.676109
52.615470	1409.053986	19.681127
52.318619	1411.882937	19.686144
52.687358	1421.109223	19.691162
52.732041	1423.707945	19.696179
52.702335	1418.400031	19.701197
53.135605	1406.435669	19.706215
52.694839	1408.421008	19.711232
52.415545	1409.377843	19.716250
52.867063	1420.977305	19.721267
53.196384	1431.215476	19.726285
53.347390	1435.297004	19.731303
53.526705	1427.916259	19.736320
53.665204	1417.602532	19.741338
53.678309	1404.068471	19.746355
53.276893	1397.644012	19.751373
53.517420	1391.809633	19.756391
53.409517	1390.907902	19.761408
53.616915	1395.541632	19.766426
53.675035	1395.969550	19.771443
53.265938	1390.334239	19.776461
53.862878	1402.252717	19.781479
53.976489	1414.650818	19.786496
53.786794	1409.880097	19.791514
53.689949	1391.744026	19.796531
53.436205	1415.411225	19.801549
54.144445	1407.552001	19.806567
53.655938	1421.719440	19.811584
53.577978	1428.098120	19.816602
53.584997	1432.241820	19.821619
53.743470	1425.169791	19.826637
54.237917	1439.856411	19.831655
53.996741	1459.000402	19.836672
54.267567	1452.570133	19.841690
54.673441	1448.934862	19.846707
54.289968	1459.515217	19.851725
54.157771	1460.160780	19.856743
54.275258	1463.176157	19.861760
54.125958	1465.805366	19.866778
54.522938	1451.871657	19.871795
54.141018	1457.227306	19.876813
54.713959	1472.966385	19.881831
54.616312	1474.871415	19.886848
54.740472	1485.326175	19.891866
54.940335	1477.288953	19.896883
55.008034	1488.572418	19.901901
55.328521	1473.910292	19.906919
55.040198	1478.650173	19.911936
54.982862	1479.945871	19.916954
54.815192	1480.410512	19.921971
55.020847	1487.369820	19.926989
55.360439	1481.096066	19.932007
55.191850	1491.728913	19.937024
55.531615	1479.609498	19.942042
55.533803	1474.480127	19.947059
55.213173	1476.314932	19.952077
55.525950	1482.589701	19.957095
55.637653	1481.606603	19.962112
55.410287	1483.652344	19.967130
55.491854	1485.250634	19.972147
55.605652	1506.143053	19.977165
56.032817	1498.014133	19.982183
55.813881	1504.675946	19.987200
55.711295	1513.106082	19.992218
56.021944	1510.163014	19.997235
56.454110	1506.583810	20.002253
56.142572	1503.257011	20.007271
56.379431	1501.070719	20.012288
56.274318	1500.247053	20.017306
56.589033	1498.642694	20.022323
56.218064	1502.555609	20.027341
56.236348	1503.352267	20.032359
56.322877	1506.528652	20.037376
56.159199	1498.231459	20.042394
56.333606	1492.228860	20.047411
56.206407	1500.936246	20.052429
56.185267	1500.040050	20.057447
56.400188	1515.776730	20.062464
56.372672	1517.840624	20.067482
56.942805	1528.749795	20.072499
56.690035	1519.982341	20.077517
56.843167	1517.975213	20.082535
56.712326	1526.455688	20.087552
56.489261	1525.333052	20.092570
56.936592	1528.454150	20.097587
57.047201	1552.903361	20.102605
57.452644	1543.069777	20.107623
57.503907	1549.421839	20.112640
57.260650	1551.288546	20.117658
57.799206	1546.067565	20.122675
57.804959	1560.745501	20.127693
58.039432	1542.713143	20.132711
57.884033	1530.485380	20.137728
57.790191	1520.559536	20.142746
57.682576	1511.558680	20.147763
57.831302	1507.931248	20.152781
58.041083	1503.220256	20.157799
58.158509	1503.460252	20.162816
57.928130	1505.437999	20.167834
58.057824	1498.577159	20.172851
57.901806	1504.518439	20.177869
57.817155	1510.344005	20.182887
58.012930	1518.396146	20.187904
57.467304	1535.326682	20.192922
57.743388	1528.118849	20.197939
57.659318	1541.839500	20.202957
57.673428	1546.247575	20.207975
57.938983	1563.609768	20.212992
58.031111	1575.215199	20.218010
58.277795	1569.315966	20.223027
58.127117	1581.046159	20.228045
58.358264	1596.932582	20.233063
58.794314	1605.189520	20.238080
58.683676	1606.510175	20.243098
59.109203	1600.875038	20.248115
59.137510	1601.164995	20.253133
58.947265	1595.462345	20.258151
59.326932	1595.172853	20.263168
59.402461	1599.860715	20.268186
59.358104	1601.593984	20.273203
59.602078	1589.272231	20.278221
59.210149	1581.536065	20.283239
59.232659	1571.303402	20.288256
59.062404	1562.117028	20.293274
59.250576	1572.596502	20.298291
59.158563	1590.852148	20.303309
58.977236	1598.601931	20.308327
59.459776	1584.763398	20.313344
59.242248	1596.625303	20.318362
59.319312	1589.734148	20.323379
59.530210	1602.477693	20.328397
59.645262	1610.146424	20.333415
60.044727	1614.963809	20.338432
59.696318	1611.807230	20.343450
59.687200	1605.300536	20.348467
59.746043	1616.762503	20.353485
59.597509	1609.606494	20.358503
60.174722	1619.539493	20.363520
60.020086	1622.585107	20.368538
60.194405	1630.283616	20.373555
60.348032	1643.964490	20.378573
60.374285	1643.697576	20.383591
60.785535	1642.626982	20.388608
60.529928	1643.893654	20.393626
60.906046	1631.915534	20.398643
60.712045	1637.963128	20.403661
60.902674	1643.607053	20.408679
61.124016	1629.680754	20.413696
60.920871	1637.775849	20.418714
60.781586	1637.506175	20.423731
60.854759	1640.180530	20.428749
60.916555	1646.531286	20.433767
61.240689	1628.115752	20.438784
61.219113	1641.121140	20.443802
61.320442	1626.824372	20.448819
61.211272	1635.172799	20.453837
60.982055	1633.310717	20.458855
61.172275	1633.511525	20.463872
60.840976	1635.060747	20.468890
61.101044	1635.852690	20.473907
61.114640	1645.031118	20.478925
61.279894	1658.327653	20.483943
61.744299	1659.692445	20.488960
61.854064	1664.841735	20.493978
62.023017	1660.410832	20.498995
62.105946	1661.546574	20.504013
61.949478	1656.197131	20.509031
62.008485	1650.658758	20.514048
61.825804	1667.157267	20.519066
62.264899	1655.175808	20.524083
62.136187	1656.913968	20.529101
61.839701	1653.740731	20.534119
61.970627	1664.164578	20.539136
61.882292	1674.771299	20.544154
62.382506	1680.277870	20.549171
62.840218	1671.684029	20.554189
62.532880	1687.662678	20.559207
62.773046	1680.479407	20.564224
62.430713	1681.830877	20.569242
62.435326	1681.004815	20.574259
62.926509	1674.828752	20.579277
62.890732	1679.037064	20.584295
63.139944	1672.508517	20.589312
63.053199	1679.428447	20.594330
63.002040	1664.979108	20.599347
63.117169	1670.459163	20.604365
62.789333	1672.022185	20.609383
63.205814	1681.544440	20.614400
63.275782	1702.319188	20.619418
63.160255	1695.089583	20.624435
63.337417	1701.197113	20.629453
63.199216	1707.898225	20.634471
63.661217	1687.861419	20.639488
63.356129	1692.293348	20.644506
63.317435	1690.548969	20.649523
63.654887	1687.063712	20.654541
63.375559	1697.618556	20.659559
63.650156	1689.645243	20.664576
63.822622	1714.676343	20.669594
63.886111	1724.686232	20.674611
64.275340	1729.072328	20.679629
64.068694	1716.140377	20.684647
64.236108	1723.775909	20.689664
64.213737	1720.115881	20.694682
64.303184	1715.845326	20.699699
64.308988	1714.651789	20.704717
64.303652	1731.133264	20.709735
64.600991	1712.799016	20.714752
64.731358	1722.317992	20.719770
64.577860	1726.824672	20.724787
64.246464	1723.885309	20.729805
64.227115	1720.434008	20.734823
64.538558	1716.947728	20.739840
64.467173	1732.505001	20.744858
64.533233	1742.288914	20.749875
64.867188	1743.307993	20.754893
64.604221	1752.206636	20.759911
64.840872	1746.683553	20.764928
65.044848	1758.438139	20.769946
65.462660	1765.313900	20.774963
65.715683	1761.791994	20.779981
65.444180	1760.645851	20.784999
65.792553	1760.405027	20.790016
65.602464	1751.582403	20.795034
65.780169	1749.850284	20.800051
65.781612	1740.265201	20.805069
65.258854	1735.593701	20.810087
65.594992	1755.326237	20.815104
65.634743	1763.010046	20.820122
65.781236	1771.710937	20.825139
65.823798	1764.924606	20.830157
65.621750	1769.434597	20.835175
65.848207	1756.542644	20.840192
66.050707	1775.960914	20.845210
66.125904	1793.122173	20.850227
66.257338	1779.805405	20.855245
66.449857	1793.126288	20.860263
66.863423	1781.548902	20.865280
66.696211	1793.270179	20.870298
66.317353	1787.403766	20.875315
66.535549	1798.038256	20.880333
66.260275	1790.477369	20.885351
66.420303	1790.799297	20.890368
66.713152	1785.813303	20.895386
66.532605	1793.965369	20.900403
67.149857	1804.379412	20.905421
67.058543	1817.740526	20.910439
66.950044	1811.504271	20.915456
67.183508	1821.984501	20.920474
67.299815	1816.430695	20.925491
67.456206	1811.413705	20.930509
67.184456	1816.540274	20.935527
67.766316	1800.004946	20.940544
67.446176	1817.018593	20.945562
67.576554	1802.113194	20.950579
67.900756	1793.824778	20.955597
67.739498	1816.466801	20.960615
67.781696	1806.243522	20.965632
67.857428	1807.757387	20.970650
67.747332	1800.749052	20.975667
67.988623	1808.466699	20.980685
67.730257	1807.355189	20.985703
67.758505	1810.129703	20.990720
68.037934	1805.377586	20.995738
67.707280	1818.215916	21.000755
68.284287	1828.023904	21.005773
68.169651	1837.947370	21.010791
68.353045	1843.237094	21.015808
68.439915	1840.640355	21.020826
68.234748	1836.787304	21.025843
68.747925	1825.554208	21.030861
68.420861	1842.844586	21.035879
68.659496	1824.590764	21.040896
68.575484	1840.129565	21.045914
68.734887	1849.219659	21.050931
69.027592	1853.714643	21.055949
69.293667	1860.102785	21.060967
69.206868	1867.897115	21.065984
69.058999	1856.690565	21.071002
69.234284	1860.067292	21.076019
69.380538	1864.348713	21.081037
69.332389	1855.866310	21.086055
69.409611	1858.314274	21.091072
69.697370	1855.305050	21.096090
69.531455	1863.780090	21.101107
69.262755	1848.006449	21.106125
69.435489	1857.482488	21.111143
69.633410	1859.751864	21.116160
69.775928	1866.183257	21.121178
69.471752	1885.332479	21.126195
69.693490	1885.820175	21.131213
69.851551	1882.105887	21.136231
70.036227	1876.201824	21.141248
70.029025	1877.640828	21.146266
70.329119	1884.026311	21.151283
70.534950	1897.608441	21.156301
70.626383	1911.714546	21.161319
70.767263	1908.981720	21.166336
70.625900	1888.234016	21.171354
70.704727	1892.560244	21.176371
71.192758	1894.546280	21.181389
70.814607	1889.507175	21.186407
70.608373	1890.458263	21.191424
71.088974	1885.989772	21.196442
70.967583	1904.390983	21.201459
70.648048	1898.139964	21.206477
71.228631	1899.353707	21.211495
70.980406	1903.611948	21.216512
71.114630	1898.360038	21.221530
71.054782	1903.932470	21.226547
71.246587	1903.024879	21.231565
71.267906	1911.990600	21.236583
71.492427	1925.976510	21.241600
71.462916	1922.922860	21.246618
71.737362	1926.526693	21.251635
71.664740	1920.498811	21.256653
72.048382	1926.834093	21.261671
71.900227	1916.056435	21.266688
72.514176	1918.100202	21.271706
72.013108	1922.339409	21.276723
72.449670	1917.426662	21.281741
72.140079	1919.880884	21.286759
72.027968	1915.921304	21.291776
72.372138	1916.484232	21.296794
72.210089	1920.055676	21.301811
72.442310	1903.070985	21.306829
72.320052	1910.975121	21.311847
72.219201	1920.752087	21.316864
72.520560	1933.205202	21.321882
72.404474	1952.979849	21.326899
72.479305	1952.352383	21.331917
72.781295	1952.041868	21.336935
72.727511	1961.190284	21.341952
72.928278	1951.814232	21.346970
72.495598	1956.149813	21.351987
73.260682	1959.456854	21.357005
73.182915	1962.977377	21.362023
73.019475	1971.048568	21.367040
73.347015	1969.047401	21.372058
73.296401	1972.115654	21.377075
73.678026	1956.940464	21.382093
73.757864	1963.566291	21.387111
73.521655	1969.400147	21.392128
73.741306	1964.122092	21.397146
73.797356	1966.421029	21.402163
73.721007	1965.559123	21.407181
73.649065	1979.562774	21.412199
73.668115	1994.039932	21.417216
73.955914	1983.960577	21.422234
73.939224	1999.456528	21.427251
74.217120	1987.786852	21.432269
74.365237	1988.933104	21.437287
74.311217	1989.821844	21.442304
74.554691	2006.214080	21.447322
74.880638	2011.576753	21.452339
74.787682	2013.696798	21.457357
74.973711	2010.537050	21.462375
74.939186	2007.579478	21.467392
75.220816	2011.157737	21.472410
74.932396	2001.631215	21.477427
75.022219	2005.416936	21.482445
74.808205	2012.403316	21.487463
75.502488	2014.016149	21.492480
75.598693	1997.440600	21.497498
75.356762	2010.184319	21.502515
75.444879	2006.022159	21.507533
75.322615	1999.094279	21.512551
75.312299	2009.399786	21.517568
75.322849	1997.663268	21.522586
75.351699	1997.612234	21.527603
75.501316	2009.891886	21.532621
75.577691	2018.095895	21.537639
75.632247	2033.988135	21.542656
76.221746	2016.132951	21.547674
76.061980	2039.216937	21.552691
76.041160	2030.650993	21.557709
76.249677	2028.685036	21.562727
76.041657	2041.588317	21.567744
76.131999	2036.768567	21.572762
76.390938	2057.497413	21.577779
76.770697	2051.542545	21.582797
76.854297	2051.353344	21.587815
76.714604	2064.766559	21.592832
77.245423	2044.552779	21.597850
76.996906	2052.112338	21.602867
76.983898	2041.125469	21.607885
77.288438	2040.634432	21.612903
77.202008	2045.310614	21.617920
77.476321	2046.897584	21.622938
77.420483	2057.400980	21.627955
77.272169	2042.867154	21.632973
77.444991	2051.264671	21.637991
77.112877	2047.779160	21.643008
77.470850	2046.592358	21.648026
77.193552	2033.612962	21.653043
77.173431	2045.689218	21.658061
77.191498	2043.627382	21.663079
77.086136	2066.616404	21.668096
77.285416	2069.871509	21.673114
77.471842	2078.401424	21.678131
77.480788	2080.264900	21.683149
77.866691	2094.046361	21.688167
77.993904	2101.818436	21.693184
78.123596	2097.376378	21.698202
78.062303	2100.667855	21.703219
78.302923	2101.604164	21.708237
78.190265	2105.330662	21.713255
78.255988	2126.004921	21.718272
78.688993	2116.612832	21.723290
78.887427	2122.270013	21.728307
79.302303	2125.985911	21.733325
79.287059	2113.119429	21.738343
79.398106	2122.569608	21.743360
79.705288	2121.910433	21.748378
79.578808	2100.780099	21.753395
79.578286	2083.798830	21.758413
79.419177	2074.289080	21.763431
79.051096	2079.815274	21.768448
79.372342	2077.953112	21.773466
79.479504	2107.490262	21.778483
79.657819	2097.993828	21.783501
79.958752	2106.645572	21.788519
79.760148	2106.550831	21.793536
79.919831	2098.796670	21.798554
79.962007	2113.183514	21.803571
79.766219	2109.621137	21.808589
79.831129	2106.955351	21.813607
79.904173	2117.337305	21.818624
79.809418	2108.136159	21.823642
79.827831	2128.049616	21.828659
80.054416	2136.533562	21.833677
80.589507	2134.915163	21.838695
80.581799	2152.119260	21.843712
80.348500	2135.656470	21.848730
80.270254	2147.239310	21.853747
80.320851	2168.334983	21.858765
80.380793	2172.080412	21.863783
80.716583	2178.822880	21.868800
80.942797	2171.912922	21.873818
80.987765	2194.038594	21.878835
81.208124	2192.010824	21.883853
81.745950	2199.179124	21.888871
81.409424	2194.706411	21.893888
81.586865	2198.345627	21.898906
81.431674	2195.980542	21.903923
81.507614	2197.827647	21.908941
81.451932	2194.848537	21.913959
81.999621	2202.712782	21.918976
82.231554	2190.173073	21.923994
82.053376	2194.230860	21.929011
82.061504	2191.909253	21.934029
81.907491	2189.515040	21.939047
82.053454	2189.147240	21.944064
82.347570	2212.442481	21.949082
82.347868	2219.271701	21.954099
82.725761	2228.770559	21.959117
82.682658	2219.657063	21.964135
82.379395	2219.835300	21.969152
82.554890	2224.989073	21.974170
82.547032	2216.889738	21.979187
82.442765	2227.683313	21.984205
82.822572	2213.697825	21.989223
82.540257	2227.774256	21.994240
82.753536	2231.051686	21.999258
82.916372	2241.502539	22.004275
82.847293	2245.737372	22.009293
83.028245	2244.378841	22.014311
82.882402	2258.166237	22.019328
83.511339	2264.052503	22.024346
83.557320	2278.100516	22.029363
83.523460	2271.738364	22.034381
83.664383	2269.115103	22.039399
83.508509	2268.101375	22.044416
83.708510	2272.350409	22.049434
83.850296	2279.272604	22.054451
83.781127	2272.152970	22.059469
84.177472	2278.591801	22.064487
84.254366	2291.761372	22.069504
84.415978	2304.068997	22.074522
84.665680	2294.930693	22.079539
84.252120	2301.687207	22.084557
84.565307	2297.848376	22.089575
84.609220	2298.753626	22.094592
84.859215	2295.714735	22.099610
84.953064	2298.672377	22.104627
84.759414	2303.191173	22.109645
84.740220	2296.787418	22.114663
84.929419	2299.213406	22.119680
84.824897	2316.616345	22.124698
85.239161	2322.876462	22.129715
85.116538	2326.215717	22.134733
85.745761	2317.476260	22.139751
85.550062	2327.332142	22.144768
85.452021	2327.733140	22.149786
85.704774	2323.387996	22.154803
85.624632	2323.797255	22.159821
86.033998	2313.387192	22.164839
85.679603	2322.730562	22.169856
86.071236	2327.858497	22.174874
86.164339	2332.108677	22.179891
86.212408	2345.229321	22.184909
86.243717	2331.243051	22.189927
86.020365	2343.739901	22.194944
86.140350	2335.025138	22.199962
86.202200	2338.755530	22.204979
86.147464	2358.276090	22.209997
86.857681	2361.190158	22.215015
86.787318	2365.612623	22.220032
86.831669	2359.790614	22.225050
87.095448	2359.808230	22.230067
86.874397	2360.677942	22.235085
87.088609	2359.998297	22.240103
87.177870	2361.611154	22.245120
87.161206	2378.661878	22.250138
87.250794	2380.738818	22.255155
87.169349	2392.854216	22.260173
87.396308	2393.606204	22.265191
87.840190	2389.150527	22.270208
87.547725	2388.114681	22.275226
87.603185	2379.982949	22.280243
87.511079	2392.773281	22.285261
88.142311	2408.771978	22.290279
88.167809	2418.112469	22.295296
88.330794	2413.823665	22.300314
88.233477	2418.870036	22.305331
87.924549	2415.648108	22.310349
88.458614	2417.697075	22.315367
88.436103	2419.988394	22.320384
88.368119	2417.932854	22.325402
88.978367	2425.355414	22.330419
88.866453	2437.198543	22.335437
88.836900	2432.606339	22.340455
88.855223	2438.136324	22.345472
88.700243	2431.292389	22.350490
89.342571	2438.624623	22.355507
89.421401	2430.192176	22.360525
89.912294	2427.444922	22.365543
89.536343	2436.244329	22.370560
89.174599	2432.454989	22.375578
89.773105	2432.779077	22.380595
89.665748	2432.131700	22.385613
89.893065	2421.652245	22.390631
89.869614	2418.985654	22.395648
89.713271	2425.216687	22.400666
89.944798	2425.114446	22.405683
89.757952	2439.741586	22.410701
90.334666	2447.713554	22.415719
90.217545	2463.774948	22.420736
89.871098	2465.849744	22.425754
90.374060	2454.871801	22.430771
90.283152	2464.886425	22.435789
90.499444	2456.113952	22.440807
90.636425	2477.186521	22.445824
90.776157	2490.580703	22.450842
90.959703	2472.378523	22.455859
90.945224	2495.851750	22.460877
91.134766	2484.363611	22.465895
91.078565	2480.570814	22.470912
90.888098	2491.106986	22.475930
91.451241	2487.731099	22.480947
91.375354	2507.222471	22.485965
91.427484	2511.479275	22.490983
91.957043	2509.838330	22.496000
91.648792	2512.283761	22.501018
92.103843	2502.891143	22.506035
92.234664	2511.116928	22.511053
92.371632	2501.093654	22.516071
92.442209	2502.934991	22.521088
91.755123	2505.512896	22.526106
92.227458	2501.689250	22.531123
92.234086	2510.897295	22.536141
92.410115	2509.034278	22.541159
92.361828	2518.622831	22.546176
92.479449	2529.295705	22.551194
92.447827	2518.740280	22.556211
92.504261	2535.307086	22.561229
92.925143	2531.889347	22.566247
92.849146	2540.055825	22.571264
92.906411	2557.918093	22.576282
93.361997	2549.475881	22.581299
93.528809	2558.228580	22.586317
93.636272	2553.812110	22.591335
93.812626	2557.523044	22.596352
93.662377	2549.248652	22.601370
94.093801	2552.841851	22.606387
93.410140	2564.583701	22.611405
93.478712	2547.280488	22.616423
93.834225	2553.223463	22.621440
93.886098	2566.807807	22.626458
93.923807	2576.958129	22.631475
93.852032	2588.143409	22.636493
94.057894	2582.413518	22.641511
94.598905	2570.295821	22.646528
94.076129	2574.452969	22.651546
94.680577	2599.312952	22.656563
94.691207	2607.405117	22.661581
95.089982	2602.062210	22.666599
95.148976	2600.549207	22.671616
95.167907	2607.553657	22.676634
95.034310	2594.951786	22.681651
94.886115	2605.906612	22.686669
95.339070	2613.745978	22.691687
95.371183	2601.415517	22.696704
95.075740	2597.211468	22.701722
95.482290	2603.070445	22.706739
95.320791	2611.360333	22.711757
95.604346	2611.914410	22.716775
96.075522	2621.034343	22.721792
95.700282	2624.267382	22.726810
96.041425	2623.106349	22.731827
96.320431	2624.808739	22.736845
96.069531	2623.968158	22.741863
96.093797	2616.186709	22.746880
96.184782	2619.982822	22.751898
96.295239	2636.248310	22.756915
96.437330	2648.469088	22.761933
96.571354	2650.411762	22.766951
96.640627	2646.411195	22.771968
96.567094	2652.917199	22.776986
96.893124	2640.982599	22.782003
97.117782	2667.582111	22.787021
97.038046	2669.282370	22.792039
97.567751	2686.598641	22.797056
97.393460	2684.424222	22.802074
97.557383	2669.952180	22.807091
97.413339	2680.357786	22.812109
97.615319	2671.898362	22.817127
97.730033	2668.309349	22.822144
97.608741	2670.734933	22.827162
97.829024	2682.099959	22.832179
97.876007	2692.084268	22.837197
98.205579	2711.334305	22.842215
98.578019	2697.231300	22.847232
98.324689	2701.344351	22.852250
98.553793	2701.421632	22.857267
98.591417	2701.647869	22.862285
98.529080	2692.784894	22.867303
98.730333	2685.747541	22.872320
98.516454	2701.741514	22.877338
98.810739	2720.197442	22.882355
98.857089	2716.459488	22.887373
98.811913	2715.107379	22.892391
99.081000	2709.663038	22.897408
99.054921	2729.806460	22.902426
99.215084	2733.163046	22.907443
99.366612	2739.228378	22.912461
99.211250	2748.427311	22.917479
99.583335	2749.068727	22.922496
99.636560	2755.182197	22.927514
100.251677	2758.162055	22.932531
100.215095	2771.557663	22.937549
100.560450	2772.964477	22.942567
100.301394	2764.524889	22.947584
100.283755	2774.753381	22.952602
100.529159	2762.584584	22.957619
100.761717	2758.868997	22.962637
100.797373	2764.152351	22.967655
100.829074	2758.034269	22.972672
100.370888	2771.703075	22.977690
100.711876	2756.745420	22.982707
100.808951	2775.576108	22.987725
100.896560	2779.226173	22.992743
101.608499	2791.911926	22.997760
101.227884	2795.131126	23.002778
101.370216	2792.790993	23.007795
101.348947	2795.911840	23.012813
101.249203	2795.686394	23.017831
101.389464	2791.854562	23.022848
101.200275	2818.950252	23.027866
101.466654	2819.210735	23.032883
101.627945	2816.711963	23.037901
101.434425	2822.759150	23.042919
102.338085	2838.292240	23.047936
102.101372	2846.266157	23.052954
102.631745	2844.560679	23.057971
102.791460	2841.896424	23.062989
102.763077	2841.750913	23.068007
102.985350	2839.420004	23.073024
102.916586	2842.206600	23.078042
103.521924	2827.944133	23.083059
103.365314	2832.166820	23.088077
103.163505	2837.683916	23.093095
103.346676	2825.973360	23.098112
103.295772	2826.437444	23.103130
103.454198	2828.439687	23.108147
103.566344	2833.854907	23.113165
103.439242	2852.896738	23.118183
103.545618	2852.211270	23.123200
103.503885	2862.717015	23.128218
103.771159	2860.191275	23.133235
103.859984	2853.381862	23.138253
103.958851	2881.151286	23.143271
104.180497	2886.794481	23.148288
104.071736	2888.579477	23.153306
104.324878	2885.760808	23.158323
104.398807	2886.202297	23.163341
104.273684	2909.425550	23.168359
104.905361	2908.566276	23.173376
105.222775	2913.221656	23.178394
105.141675	2899.109163	23.183411
105.699163	2907.244777	23.188429
105.220900	2907.744048	23.193447
105.528249	2894.774399	23.198464
105.520114	2915.180045	23.203482
105.471742	2907.975582	23.208499
105.915525	2905.816712	23.213517
105.752273	2902.862523	23.218535
105.947211	2886.893888	23.223552
105.848265	2919.769435	23.228570
105.690945	2924.585149	23.233587
106.244096	2931.475096	23.238605
106.129795	2931.915801	23.243623
106.489904	2932.372206	23.248640
106.262750	2936.547131	23.253658
106.452329	2942.902699	23.258675
106.603678	2951.962100	23.263693
106.533615	2956.396100	23.268711
106.828900	2950.217853	23.273728
106.799241	2957.271433	23.278746
106.820314	2958.957823	23.283763
107.092331	2974.468657	23.288781
106.997703	2992.661630	23.293799
107.503215	2983.481045	23.298816
107.671817	2985.393049	23.303834
107.793525	2990.528803	23.308851
108.086738	2981.588015	23.313869
108.088796	2992.932638	23.318887
108.149435	2977.921494	23.323904
108.226380	2981.774935	23.328922
108.004217	2990.831907	23.333939
108.343858	3001.718410	23.338957
108.520656	3000.630765	23.343975
108.688907	3009.619693	23.348992
108.818021	3010.237493	23.354010
108.918486	3000.958480	23.359027
108.929178	3002.254480	23.364045
108.880179	3004.456762	23.369063
108.925056	3001.677603	23.374080
109.448288	3002.364525	23.379098
109.191485	2999.585218	23.384115
109.195932	2995.660428	23.389133
109.055763	3009.437516	23.394151
109.218582	3028.413547	23.399168
109.402649	3029.081319	23.404186
109.417971	3033.895704	23.409203
109.499512	3034.776080	23.414221
109.439995	3058.819785	23.419239
110.255880	3057.387567	23.424256
110.078767	3052.606578	23.429274
109.810142	3064.547140	23.434291
110.356197	3069.281319	23.439309
110.177443	3083.744350	23.444327
110.373342	3081.487445	23.449344
110.638965	3080.839825	23.454362
110.871554	3081.088575	23.459379
111.688914	3090.837976	23.464397
111.518414	3080.503336	23.469415
111.527407	3082.140556	23.474432
111.624607	3065.998918	23.479450
111.466308	3063.672202	23.484467
111.998796	3083.385217	23.489485
111.721565	3091.920658	23.494503
111.479802	3089.651035	23.499520
111.855274	3083.765380	23.504538
112.027703	3090.259270	23.509555
112.515017	3078.190012	23.514573
112.301562	3095.271681	23.519591
112.022441	3086.242340	23.524608
112.529798	3095.516217	23.529626
112.957284	3123.183746	23.534643
113.117740	3104.089593	23.539661
112.757156	3119.853129	23.544679
112.815864	3115.909894	23.549696
112.884362	3118.998651	23.554714
112.232338	3120.196694	23.559731
113.316000	3135.529089	23.564749
113.329236	3144.941728	23.569767
113.423408	3146.477482	23.574784
113.190491	3148.834580	23.579802
113.276727	3146.753655	23.584819
113.797723	3163.777818	23.589837
113.407906	3173.396439	23.594855
113.812780	3173.242719	23.599872
113.759739	3179.812091	23.604890
113.823299	3201.076317	23.609907
114.296869	3206.009518	23.614925
114.174583	3216.625661	23.619943
114.362647	3203.903018	23.624960
114.613013	3217.444505	23.629978
114.913173	3229.915601	23.634995
114.997690	3225.651547	23.640013
115.336191	3234.616411	23.645031
115.348686	3229.031223	23.650048
115.195569	3233.212892	23.655066
115.355531	3228.117102	23.660083
115.544615	3235.875983	23.665101
115.623021	3256.832723	23.670119
115.884034	3255.042974	23.675136
115.889319	3263.096405	23.680154
115.812573	3256.262994	23.685171
115.925917	3256.363345	23.690189
115.857364	3254.832772	23.695207
116.062472	3267.682587	23.700224
116.480974	3285.992686	23.705242
116.168679	3292.582897	23.710259
116.624862	3286.839338	23.715277
116.882978	3285.132740	23.720295
116.745202	3290.008328	23.725312
116.880518	3284.430384	23.730330
116.527381	3317.786561	23.735347
116.886467	3315.039283	23.740365
116.957574	3319.603993	23.745383
116.865101	3330.533391	23.750400
117.177585	3336.468821	23.755418
117.116122	3352.605205	23.760435
117.893719	3342.684190	23.765453
118.026409	3374.446071	23.770471
117.833060	3372.226672	23.775488
118.223712	3369.378108	23.780506
117.941033	3377.853976	23.785523
118.062359	3369.853162	23.790541
118.657997	3383.135384	23.795559
118.687308	3395.006497	23.800576
118.785023	3389.583151	23.805594
119.029964	3397.149028	23.810611
119.331263	3399.607258	23.815629
119.363088	3392.826318	23.820647
119.289943	3390.749256	23.825664
119.265659	3393.645529	23.830682
119.065452	3407.562021	23.835699
119.282880	3408.932555	23.840717
119.749947	3428.050138	23.845735
119.640288	3420.645724	23.850752
119.803438	3415.195809	23.855770
120.091741	3436.867704	23.860787
120.383092	3445.623162	23.865805
120.390627	3456.811710	23.870823
119.984661	3453.527053	23.875840
120.538185	3453.858211	23.880858
120.196231	3455.576294	23.885875
120.565448	3470.528659	23.890893
120.894073	3476.917376	23.895911
121.146029	3471.624025	23.900928
121.284453	3475.229639	23.905946
120.905402	3484.151799	23.910963
121.538984	3500.931355	23.915981
121.665278	3506.316520	23.920999
121.472094	3508.787577	23.926016
122.035104	3507.841592	23.931034
121.757937	3519.129196	23.936051
122.037942	3512.359164	23.941069
122.286479	3508.738790	23.946087
122.302634	3526.816840	23.951104
122.618584	3524.642791	23.956122
122.672310	3533.520240	23.961139
122.792324	3519.212534	23.966157
123.226811	3517.639366	23.971175
123.095157	3524.723443	23.976192
123.318428	3518.845452	23.981210
123.132434	3524.785763	23.986227
123.106057	3513.296716	23.991245
123.116566	3528.756830	23.996263
123.052124	3549.404501	24.001280
123.575387	3546.119429	24.006298
123.477791	3554.431347	24.011315
123.731937	3548.380134	24.016333
123.938259	3563.075649	24.021351
123.910442	3573.878787	24.026368
123.925714	3579.889012	24.031386
124.059965	3587.107133	24.036403
123.917181	3580.567560	24.041421
124.347810	3606.232688	24.046439
124.434107	3611.889065	24.051456
125.010262	3603.809827	24.056474
124.936706	3610.491431	24.061491
124.776488	3614.564532	24.066509
124.854179	3624.002638	24.071527
124.850200	3629.812521	24.076544
125.391082	3632.402067	24.081562
125.521677	3642.288134	24.086579
125.558339	3647.172805	24.091597
125.795144	3655.908262	24.096615
125.616465	3669.755290	24.101632
125.945878	3662.834903	24.106650
126.203872	3672.666080	24.111667
126.713686	3668.067458	24.116685
126.655345	3662.867835	24.121703
126.352118	3670.692533	24.126720
126.195059	3679.395446	24.131738
126.846245	3685.652211	24.136755
126.938953	3694.525673	24.141773
126.702956	3697.371945	24.146791
126.703759	3713.813770	24.151808
127.116204	3716.123764	24.156826
127.264733	3724.378175	24.161843
127.004425	3734.848973	24.166861
127.662830	3742.464024	24.171879
127.555177	3747.016665	24.176896
127.986529	3743.028627	24.181914
128.563201	3754.615082	24.186931
128.813033	3758.943303	24.191949
128.817315	3736.273765	24.196967
128.298252	3748.691667	24.201984
128.824460	3758.209682	24.207002
129.072487	3767.986268	24.212019
128.973268	3769.175295	24.217037
129.335375	3758.856135	24.222055
129.176730	3764.849499	24.227072
129.251864	3760.927009	24.232090
129.319380	3772.058235	24.237107
128.779271	3776.457143	24.242125
129.519476	3788.157155	24.247143
129.197664	3802.264961	24.252160
129.855836	3807.213524	24.257178
130.096903	3823.387811	24.262195
129.670465	3838.316095	24.267213
130.447295	3823.420836	24.272231
130.337039	3837.660648	24.277248
130.469523	3839.901959	24.282266
130.625258	3858.790018	24.287283
130.801992	3862.623253	24.292301
131.028628	3853.256348	24.297319
131.050558	3854.766707	24.302336
131.328221	3860.028558	24.307354
131.290891	3879.496975	24.312371
131.357423	3889.566229	24.317389
131.237493	3881.751475	24.322407
131.458410	3884.243145	24.327424
132.103918	3896.421885	24.332442
132.080661	3910.211161	24.337459
131.949544	3913.437786	24.342477
132.347990	3912.078413	24.347495
132.259337	3913.696421	24.352512
132.045434	3901.892003	24.357530
132.263219	3915.995005	24.362547
132.688149	3945.539258	24.367565
132.915645	3941.578555	24.372583
132.989000	3940.513057	24.377600
133.219822	3946.677968	24.382618
133.383703	3959.613518	24.387635
133.317354	3957.126194	24.392653
133.619462	3956.641806	24.397671
133.547309	3958.159453	24.402688
133.685917	3940.272632	24.407706
134.122180	3955.524630	24.412723
134.388279	3969.377173	24.417741
134.513669	3977.262700	24.422759
134.463942	4003.862600	24.427776
134.424281	3991.426554	24.432794
134.467230	3986.948290	24.437811
134.591073	3986.005552	24.442829
134.881899	3983.942287	24.447847
134.662289	3987.482767	24.452864
135.035995	4005.739308	24.457882
135.458358	4016.359704	24.462899
135.358377	4017.739826	24.467917
135.325111	4017.004152	24.472935
135.051756	4026.154437	24.477952
135.579908	4035.951048	24.482970
135.564414	4046.277270	24.487987
135.663200	4064.465917	24.493005
136.205849	4067.943065	24.498023
135.832828	4073.266045	24.503040
136.088003	4085.476360	24.508058
136.313609	4095.081261	24.513075
136.708165	4104.418876	24.518093
136.662894	4097.289334	24.523111
137.175926	4123.139739	24.528128
137.189213	4124.497217	24.533146
137.348035	4130.577246	24.538163
137.483718	4126.383628	24.543181
137.940876	4127.391771	24.548199
137.664440	4139.608470	24.553216
137.631592	4154.839355	24.558234
137.773565	4162.824602	24.563251
138.060851	4161.504442	24.568269
137.715256	4166.131168	24.573287
138.085980	4181.733205	24.578304
138.385904	4191.434946	24.583322
138.828555	4188.248499	24.588339
138.537695	4205.236690	24.593357
139.102375	4206.954264	24.598375
139.353917	4209.033825	24.603392
139.350714	4211.911805	24.608410
139.603908	4206.699895	24.613427
139.500482	4224.628824	24.618445
140.015065	4231.061934	24.623463
139.939263	4240.659246	24.628480
140.263566	4235.136747	24.633498
140.005505	4240.738044	24.638515
140.082804	4235.296911	24.643533
140.331892	4231.360521	24.648551
140.604064	4261.247557	24.653568
140.563408	4268.832309	24.658586
141.241512	4270.944551	24.663603
140.842535	4278.544419	24.668621
140.959557	4267.192150	24.673639
140.945098	4290.156255	24.678656
141.031278	4298.716955	24.683674
141.433350	4304.027302	24.688691
141.030305	4304.700013	24.693709
141.695733	4311.814954	24.698727
141.734165	4324.559322	24.703744
141.796022	4332.619314	24.708762
141.959586	4345.251287	24.713779
142.199017	4348.447090	24.718797
142.195680	4340.193531	24.723815
142.351215	4359.083806	24.728832
142.755011	4370.246907	24.733850
143.075319	4384.035742	24.738867
143.007743	4390.265491	24.743885
143.366181	4382.359237	24.748903
143.228819	4386.095282	24.753920
143.273181	4381.076095	24.758938
143.425638	4388.988463	24.763955
143.386461	4405.346675	24.768973
143.708568	4406.992537	24.773991
143.491887	4405.599323	24.779008
144.384862	4432.080410	24.784026
144.471204	4428.903968	24.789043
144.418439	4426.421018	24.794061
145.195737	4442.046299	24.799079
144.868246	4432.628475	24.804096
144.799273	4430.279704	24.809114
144.977367	4442.130183	24.814131
144.859693	4456.581244	24.819149
145.066186	4466.908468	24.824167
145.065062	4469.829068	24.829184
145.375929	4482.763602	24.834202
145.587129	4495.377982	24.839219
145.432713	4498.452663	24.844237
145.770686	4511.344944	24.849255
146.150959	4519.849297	24.854272
146.110429	4520.696776	24.859290
146.335574	4531.020961	24.864307
146.645104	4545.027480	24.869325
146.855180	4545.619367	24.874343
146.882155	4551.460701	24.879360
147.050011	4555.042018	24.884378
147.451944	4569.045102	24.889395
147.362652	4573.854414	24.894413
147.522175	4573.938483	24.899431
147.567381	4575.784456	24.904448
147.663307	4588.101011	24.909466
148.085150	4597.321810	24.914483
148.024515	4602.450036	24.919501
148.325046	4607.109509	24.924519
148.527411	4607.574318	24.929536
148.755539	4620.247818	24.934554
149.223530	4627.077399	24.939571
149.259855	4630.726138	24.944589
149.340350	4630.506710	24.949607
149.089389	4626.286682	24.954624
149.247646	4622.543954	24.959642
149.350513	4636.796921	24.964659
149.324496	4648.858459	24.969677
149.696015	4656.591451	24.974695
149.857336	4662.096829	24.979712
149.885588	4685.480471	24.984730
150.512272	4685.740517	24.989747
150.270462	4693.194135	24.994765
150.347378	4693.448558	24.999783
150.650673	4699.673059	25.004800
150.350928	4721.633293	25.009818
150.657614	4722.240723	25.014835
150.849160	4727.928150	25.019853
151.369757	4734.401425	25.024871
151.326087	4743.995312	25.029888
151.265555	4756.309897	25.034906
151.685890	4762.880858	25.039923
152.195194	4774.336288	25.044941
152.165758	4784.075103	25.049959
152.620903	4772.548873	25.054976
152.298124	4781.033306	25.059994
152.779581	4774.499149	25.065011
152.695193	4769.959017	25.070029
152.731085	4776.179698	25.075047
152.776224	4781.959452	25.080064
153.128173	4792.057331	25.085082
153.328562	4801.430599	25.090099
153.392856	4808.999061	25.095117
153.156176	4801.170455	25.100135
153.784706	4823.395987	25.105152
153.361212	4829.145702	25.110170
154.027576	4830.127597	25.115187
154.057104	4834.178324	25.120205
154.188054	4843.721371	25.125223
154.369747	4852.528818	25.130240
154.391364	4849.409840	25.135258
154.632053	4856.313303	25.140275
154.500498	4869.916582	25.145293
154.553823	4878.459799	25.150311
155.043364	4887.624700	25.155328
155.192595	4895.491398	25.160346
155.422300	4919.838246	25.165363
155.616418	4923.552721	25.170381
155.518316	4919.992056	25.175399
155.864038	4935.862783	25.180416
155.912745	4940.547429	25.185434
156.287891	4939.294586	25.190451
156.547773	4946.977266	25.195469
156.479639	4962.345488	25.200487
157.125445	4962.087379	25.205504
157.097577	4963.860819	25.210522
157.188773	4962.120595	25.215539
157.670593	4961.443088	25.220557
157.432489	4973.962790	25.225575
157.723667	4975.098033	25.230592
157.808804	5003.611373	25.235610
157.926116	4987.844770	25.240627
157.964505	4995.233334	25.245645
157.937453	5012.373710	25.250663
158.193624	5018.816774	25.255680
158.073377	5013.686382	25.260698
158.546615	5036.233965	25.265715
158.683656	5050.920679	25.270733
159.028436	5056.892779	25.275751
159.287055	5050.689448	25.280768
159.084837	5069.498738	25.285786
159.615548	5071.701991	25.290803
159.593244	5081.648886	25.295821
159.357398	5093.775361	25.300839
160.002167	5104.204623	25.305856
160.004595	5118.984910	25.310874
160.080110	5112.269633	25.315891
160.665525	5120.356133	25.320909
160.486088	5134.499492	25.325927
160.865927	5133.815598	25.330944
160.874469	5136.457928	25.335962
161.095546	5124.718911	25.340979
161.132938	5159.800882	25.345997
160.986029	5164.730535	25.351015
161.358963	5167.645370	25.356032
161.807029	5187.794739	25.361050
161.930855	5182.757835	25.366067
162.034134	5191.929645	25.371085
161.830626	5199.596487	25.376103
162.033387	5210.342185	25.381120
162.207923	5221.545355	25.386138
162.433399	5225.655155	25.391155
162.946386	5231.260125	25.396173
163.276932	5251.628621	25.401191
163.634246	5244.530077	25.406208
163.383711	5242.665166	25.411226
163.717935	5239.581869	25.416243
163.911630	5244.269818	25.421261
163.963063	5242.434154	25.426279
164.138163	5226.764072	25.431296
164.086132	5250.458705	25.436314
164.485705	5261.236492	25.441331
164.731843	5265.014903	25.446349
164.295637	5284.555703	25.451367
164.820170	5270.601647	25.456384
164.622644	5286.281754	25.461402
164.603634	5288.842038	25.466419
165.094254	5295.938284	25.471437
164.795728	5306.116414	25.476455
165.403750	5322.921464	25.481472
165.386714	5333.825624	25.486490
165.824512	5347.038755	25.491507
165.860194	5357.414480	25.496525
165.903738	5364.978765	25.501543
166.210132	5373.574543	25.506560
166.240050	5394.599657	25.511578
166.190186	5382.761105	25.516595
166.788844	5415.997176	25.521613
166.953826	5410.552566	25.526631
167.337938	5412.037095	25.531648
167.814079	5435.334861	25.536666
167.690257	5446.467004	25.541683
168.137604	5441.868743	25.546701
167.849345	5446.539524	25.551719
168.284853	5450.940702	25.556736
167.998945	5453.646305	25.561754
168.088598	5464.309674	25.566771
168.667154	5472.774702	25.571789
168.438969	5485.409721	25.576807
168.799370	5497.918756	25.581824
168.642614	5510.094302	25.586842
168.978941	5527.308287	25.591859
169.376732	5527.232902	25.596877
169.273566	5542.987449	25.601895
169.716569	5554.078774	25.606912
170.070194	5565.842830	25.611930
170.271255	5575.029028	25.616947
170.353646	5574.345832	25.621965
170.247122	5595.666628	25.626983
170.427461	5607.671972	25.632000
170.568211	5611.167055	25.637018
170.912137	5625.814219	25.642035
171.360900	5628.664245	25.647053
171.678326	5632.375448	25.652071
171.926985	5614.947723	25.657088
172.095368	5628.146545	25.662106
172.334016	5637.544707	25.667123
172.423608	5644.632561	25.672141
172.300936	5654.495209	25.677159
172.533306	5650.413966	25.682176
172.591689	5651.463695	25.687194
172.567893	5648.341824	25.692212
172.946399	5678.137223	25.697229
173.032226	5685.501344	25.702247
173.125408	5683.318923	25.707264
173.019990	5691.147773	25.712282
173.235808	5720.609062	25.717300
173.824461	5721.943276	25.722317
173.717056	5731.504592	25.727335
173.860321	5747.798231	25.732352
173.755198	5759.809120	25.737370
174.046528	5761.554716	25.742388
174.326747	5767.045171	25.747405
174.139532	5775.709342	25.752423
174.470331	5783.753997	25.757440
174.693760	5806.475089	25.762458
174.504688	5811.246534	25.767476
175.124038	5828.027420	25.772493
175.240730	5840.198991	25.777511
175.779288	5854.061745	25.782528
175.841064	5869.609420	25.787546
175.816420	5872.242000	25.792564
175.925084	5875.503040	25.797581
176.287265	5901.305721	25.802599
176.379320	5903.708758	25.807616
176.343203	5920.050722	25.812634
176.335770	5936.042637	25.817652
176.816129	5944.048882	25.822669
176.722576	5958.644608	25.827687
177.319480	5977.833260	25.832704
177.699037	5989.129895	25.837722
177.704534	5997.665088	25.842740
178.226420	5996.244986	25.847757
178.286213	6015.117644	25.852775
178.320186	6022.499942	25.857792
178.631019	6024.245890	25.862810
178.817949	6040.806676	25.867828
178.986581	6052.042917	25.872845
178.723672	6063.303218	25.877863
178.908645	6063.190938	25.882880
179.311930	6076.382433	25.887898
179.702892	6088.767188	25.892916
180.069517	6095.875625	25.897933
180.052220	6117.711209	25.902951
180.214257	6117.865752	25.907968
180.473657	6114.998225	25.912986
180.465806	6139.766596	25.918004
180.708738	6147.321546	25.923021
180.583509	6156.418668	25.928039
181.255479	6168.230988	25.933056
181.304713	6186.020383	25.938074
181.142316	6178.944683	25.943092
181.640555	6185.427381	25.948109
181.737430	6219.649395	25.953127
181.751859	6212.257015	25.958144
181.858022	6238.313215	25.963162
182.480880	6246.946572	25.968180
183.077604	6236.103086	25.973197
182.815761	6253.242266	25.978215
183.044035	6258.422920	25.983232
183.318878	6267.769016	25.988250
183.095770	6264.539380	25.993268
183.688198	6283.999271	25.998285
183.600044	6296.475167	26.003303
183.520733	6299.386581	26.008320
183.757160	6307.224620	26.013338
183.759914	6330.454273	26.018356
184.627383	6336.992583	26.023373
184.817112	6348.846130	26.028391
184.893111	6350.195409	26.033408
185.441428	6340.536430	26.038426
185.451745	6358.374977	26.043444
186.078552	6366.154058	26.048461
185.749120	6376.958564	26.053479
185.916340	6372.142102	26.058496
186.106778	6378.931688	26.063514
185.907097	6379.638998	26.068532
186.125688	6385.765553	26.073549
186.340047	6410.279488	26.078567
186.667287	6405.711427	26.083584
186.800906	6403.267064	26.088602
186.597692	6426.570267	26.093620
186.874633	6437.537664	26.098637
187.228464	6452.238700	26.103655
187.361897	6460.775057	26.108672
187.648084	6474.021675	26.113690
187.413330	6478.050340	26.118708
188.077314	6497.692410	26.123725
188.011908	6511.146784	26.128743
188.069617	6517.695320	26.133760
188.365082	6533.173932	26.138778
188.217983	6544.103573	26.143796
188.897403	6553.457023	26.148813
188.961211	6567.371286	26.153831
188.911964	6578.376138	26.158848
189.408105	6602.444528	26.163866
189.520809	6607.263220	26.168884
190.128143	6616.946001	26.173901
189.974754	6632.933601	26.178919
190.038217	6634.598421	26.183936
190.693314	6655.425847	26.188954
190.429603	6658.932470	26.193972
190.928516	6674.337441	26.198989
191.152109	6697.485469	26.204007
191.471483	6694.149573	26.209024
191.493710	6704.483521	26.214042
191.406440	6727.430938	26.219060
191.787775	6718.997191	26.224077
192.329605	6732.134846	26.229095
192.314749	6749.633834	26.234112
192.108147	6748.521472	26.239130
192.069897	6772.403561	26.244148
192.814314	6780.064972	26.249165
193.059297	6796.516944	26.254183
192.856677	6805.816241	26.259200
193.169005	6819.070644	26.264218
193.210198	6840.745567	26.269236
193.770534	6837.987276	26.274253
193.352422	6864.012215	26.279271
193.555824	6878.317947	26.284288
194.153581	6900.298713	26.289306
194.604448	6919.057437	26.294324
194.895423	6917.724239	26.299341
195.124674	6940.291254	26.304359
195.499931	6931.018854	26.309376
195.946853	6922.066970	26.314394
195.551378	6939.016331	26.319412
196.342241	6951.538100	26.324429
196.047381	6962.944507	26.329447
196.335994	6968.865192	26.334464
196.636215	6971.091843	26.339482
196.888439	6989.994520	26.344500
196.922146	6994.751564	26.349517
196.756815	6987.465702	26.354535
196.857435	7018.265274	26.359552
197.485361	7028.247335	26.364570
197.304827	7033.935257	26.369588
197.554983	7037.290116	26.374605
197.552833	7063.160809	26.379623
197.756370	7078.387373	26.384640
198.079758	7097.094915	26.389658
198.502334	7108.753837	26.394676
198.634926	7119.695156	26.399693
199.002490	7129.756529	26.404711
199.110864	7142.581809	26.409728
199.419153	7149.518435	26.414746
199.675815	7156.273789	26.419764
199.741317	7169.066007	26.424781
199.718062	7179.329023	26.429799
200.000142	7198.034060	26.434816
200.269908	7197.550991	26.439834
200.060884	7212.229175	26.444852
200.326769	7232.477434	26.449869
200.854929	7226.607938	26.454887
200.728857	7246.223967	26.459904
201.141613	7255.205267	26.464922
201.172828	7277.792097	26.469940
201.140571	7278.221331	26.474957
201.881651	7298.984213	26.479975
201.655069	7316.309314	26.484992
201.975378	7316.219560	26.490010
202.158053	7348.212797	26.495028
202.547596	7345.424359	26.500045
203.061711	7362.761808	26.505063
202.888009	7373.579854	26.510080
203.130705	7387.611777	26.515098
203.276840	7402.152697	26.520116
203.389154	7408.053846	26.525133
203.538281	7419.818824	26.530151
203.877117	7426.955299	26.535168
204.388740	7451.428829	26.540186
204.290507	7462.873203	26.545204
204.720779	7472.477870	26.550221
205.015340	7488.093038	26.555239
204.900498	7501.227997	26.560256
204.974517	7504.473442	26.565274
205.566092	7528.698391	26.570292
205.709302	7525.637159	26.575309
206.058094	7547.716673	26.580327
205.646349	7564.369315	26.585344
206.618165	7575.385731	26.590362
206.587675	7589.903238	26.595380
206.663296	7608.128571	26.600397
207.115114	7621.985170	26.605415
207.138519	7630.697074	26.610432
207.448138	7634.203695	26.615450
207.368322	7653.033648	26.620468
207.904927	7670.812716	26.625485
207.897415	7664.726762	26.630503
207.834948	7687.611618	26.635520
208.184296	7707.418241	26.640538
208.739605	7718.739855	26.645556
208.771018	7736.078708	26.650573
209.121166	7735.352364	26.655591
209.281078	7752.822800	26.660608
209.611797	7751.035608	26.665626
209.668531	7768.016677	26.670644
209.709059	7784.160064	26.675661
210.266378	7790.049266	26.680679
210.376670	7816.749294	26.685696
210.717920	7819.608829	26.690714
211.105049	7841.428022	26.695732
210.975128	7849.616414	26.700749
210.876022	7852.477827	26.705767
210.943712	7874.258481	26.710784
211.509285	7882.339855	26.715802
211.613572	7904.724904	26.720820
211.816108	7920.217085	26.725837
212.299296	7931.120731	26.730855
212.325519	7948.019609	26.735872
212.445737	7952.016776	26.740890
212.415577	7974.977045	26.745908
212.866669	7985.485134	26.750925
213.141185	8002.110699	26.755943
213.465037	8019.522839	26.760960
213.714859	8011.922174	26.765978
214.418593	8043.523557	26.770996
214.235459	8037.313679	26.776013
214.550706	8049.400595	26.781031
214.412334	8053.941439	26.786048
214.971633	8066.596089	26.791066
215.192501	8081.149704	26.796084
215.181221	8079.175606	26.801101
215.247803	8095.930140	26.806119
215.214126	8116.712629	26.811136
215.514528	8122.549102	26.816154
216.004416	8135.934378	26.821172
215.593882	8148.639851	26.826189
216.283484	8173.877448	26.831207
216.393791	8196.407626	26.836224
216.718355	8197.259960	26.841242
216.793792	8208.106722	26.846260
217.215073	8243.679143	26.851277
217.240607	8251.563236	26.856295
217.241162	8266.792191	26.861312
217.398032	8278.662859	26.866330
218.204644	8288.881635	26.871348
218.307892	8305.501161	26.876365
219.036463	8303.972681	26.881383
218.938371	8329.724248	26.886400
218.894682	8336.130402	26.891418
218.996436	8355.013891	26.896436
219.159675	8362.507462	26.901453
219.603601	8373.680973	26.906471
219.899421	8402.284198	26.911488
220.244980	8415.573049	26.916506
220.620302	8428.805797	26.921524
220.526233	8438.719014	26.926541
221.041496	8467.180556	26.931559
220.683375	8478.229097	26.936576
220.731287	8497.883302	26.941594
221.799542	8500.262106	26.946612
221.695020	8507.326611	26.951629
222.015181	8521.094696	26.956647
222.143120	8539.435330	26.961664
222.340810	8555.423574	26.966682
222.600214	8580.597424	26.971700
222.592816	8589.030603	26.976717
223.058023	8599.436739	26.981735
223.058555	8609.748736	26.986752
223.111087	8628.952593	26.991770
223.521088	8648.743286	26.996788
223.566914	8664.212465	27.001805
224.106854	8684.207002	27.006823
223.992710	8699.459260	27.011840
224.291779	8718.999779	27.016858
224.653592	8730.035092	27.021876
224.476856	8758.672927	27.026893
225.018099	8773.343591	27.031911
225.266551	8791.162079	27.036928
225.172762	8798.729828	27.041946
225.609954	8822.367109	27.046964
225.892443	8848.667073	27.051981
225.966879	8866.146558	27.056999
226.365132	8885.541719	27.062016
227.049366	8898.059034	27.067034
227.265461	8904.857286	27.072052
227.422093	8929.720213	27.077069
227.935825	8919.328926	27.082087
228.114443	8949.691665	27.087104
228.343113	8961.076019	27.092122
228.544218	8965.672095	27.097140
228.279842	8976.164364	27.102157
228.598526	8981.487727	27.107175
228.787215	9000.745941	27.112192
228.678874	9000.014165	27.117210
229.273943	9024.826070	27.122228
229.298890	9040.949680	27.127245
229.656055	9054.412801	27.132263
229.886525	9083.196612	27.137280
229.850792	9091.759191	27.142298
230.773306	9101.348115	27.147316
230.395229	9127.589118	27.152333
230.869941	9133.849292	27.157351
231.129103	9146.474056	27.162368
231.033946	9166.332316	27.167386
231.650755	9190.001907	27.172404
231.611862	9205.746331	27.177421
231.694124	9220.476702	27.182439
232.270624	9241.338651	27.187456
232.442116	9246.729745	27.192474
232.590428	9269.991649	27.197492
232.591406	9280.268561	27.202509
233.105461	9301.515056	27.207527
233.189408	9315.611151	27.212544
233.205022	9334.696718	27.217562
233.717162	9358.847013	27.222580
233.992113	9375.826044	27.227597
234.209162	9392.692568	27.232615
234.448563	9414.502891	27.237632
234.585055	9442.421454	27.242650
234.823908	9446.375767	27.247668
235.092140	9470.502728	27.252685
235.362189	9482.933763	27.257703
235.784020	9498.903255	27.262720
236.075581	9534.644150	27.267738
236.739796	9535.708260	27.272756
236.403004	9552.883074	27.277773
236.695427	9555.216150	27.282791
236.710734	9583.870999	27.287808
237.333804	9604.316917	27.292826
237.284243	9612.743425	27.297844
237.444817	9630.213457	27.302861
237.827328	9630.696320	27.307879
238.165084	9660.818294	27.312896
238.415386	9677.301528	27.317914
239.302456	9684.604453	27.322932
239.153772	9691.161621	27.327949
239.754273	9706.046280	27.332967
239.851494	9722.716333	27.337984
239.622980	9720.212351	27.343002
240.090375	9745.745171	27.348020
240.038964	9759.689940	27.353037
240.074376	9774.655423	27.358055
240.600272	9795.248402	27.363072
240.279365	9829.710296	27.368090
240.906352	9834.018854	27.373108
241.185387	9852.815753	27.378125
241.498268	9880.866636	27.383143
241.720702	9894.060488	27.388160
241.744758	9910.260744	27.393178
242.339299	9929.876031	27.398196
241.860789	9955.392170	27.403213
242.015287	9968.019124	27.408231
242.579626	9993.625337	27.413248
242.602683	10023.637720	27.418266
243.319411	10035.422717	27.423284
243.736993	10055.785009	27.428301
243.959518	10072.678918	27.433319
244.322592	10085.065122	27.438336
244.514473	10103.507274	27.443354
244.597256	10110.591956	27.448372
244.999746	10126.511709	27.453389
245.004412	10139.665334	27.458407
245.460779	10168.195584	27.463424
245.403607	10176.491309	27.468442
245.694793	10194.459490	27.473460
246.064677	10216.338366	27.478477
246.174585	10234.717016	27.483495
246.097779	10252.954810	27.488512
246.309026	10275.761140	27.493530
246.721127	10293.577905	27.498548
246.968296	10310.675956	27.503565
247.194115	10332.968722	27.508583
247.674559	10353.139040	27.513600
247.700279	10376.403119	27.518618
248.035910	10399.074852	27.523636
248.177037	10417.753409	27.528653
248.462226	10440.023911	27.533671
248.571965	10461.376567	27.538688
249.076123	10480.923966	27.543706
249.404320	10504.321799	27.548724
249.584199	10527.221110	27.553741
249.965097	10546.324184	27.558759
250.273711	10564.094542	27.563776
250.385544	10587.547938	27.568794
250.637045	10581.319609	27.573812
251.131620	10612.361190	27.578829
251.222863	10627.716848	27.583847
251.537161	10649.977319	27.588864
252.151051	10663.333217	27.593882
252.417553	10675.909928	27.598900
252.260736	10701.322112	27.603917
252.705821	10710.877463	27.608935
252.912766	10725.838340	27.613952
253.015674	10743.809100	27.618970
253.433506	10761.593143	27.623988
253.477886	10786.297114	27.629005
253.747036	10797.102607	27.634023
254.004011	10818.368393	27.639040
254.222178	10832.782388	27.644058
254.830098	10850.406720	27.649076
255.174286	10871.637686	27.654093
255.367313	10880.856658	27.659111
255.673801	10900.426200	27.664128
255.848966	10927.924244	27.669146
256.116493	10932.089251	27.674164
256.090874	10946.883940	27.679181
256.295185	10966.162428	27.684199
256.924621	10983.146050	27.689216
257.030017	11011.567210	27.694234
257.354955	11015.647128	27.699252
257.431574	11037.832392	27.704269
257.722257	11050.366015	27.709287
257.999959	11080.970100	27.714304
258.196752	11096.467898	27.719322
258.577590	11110.102946	27.724340
258.748108	11134.742498	27.729357
258.777311	11152.732983	27.734375
259.422876	11178.520684	27.739392
259.472071	11201.842740	27.744410
259.928619	11211.629680	27.749428
259.853335	11232.185977	27.754445
260.581458	11245.191049	27.759463
260.662086	11267.852575	27.764480
260.585716	11284.622260	27.769498
260.779023	11300.775478	27.774516
261.051790	11323.370677	27.779533
261.384395	11336.932745	27.784551
261.797136	11369.173354	27.789568
261.751160	11384.938422	27.794586
262.001347	11404.528123	27.799604
262.232562	11424.109166	27.804621
262.423885	11445.986926	27.809639
262.918187	11468.552031	27.814656
262.783233	11497.566788	27.819674
262.995893	11502.770653	27.824692
263.703693	11537.165518	27.829709
264.173974	11564.662375	27.834727
264.887131	11563.949164	27.839744
264.774155	11591.291122	27.844762
265.317474	11607.333252	27.849780
265.548638	11611.183812	27.854797
265.471252	11636.998732	27.859815
265.797500	11640.715420	27.864832
266.103207	11668.848614	27.869850
266.057400	11680.362976	27.874868
266.507519	11704.391568	27.879885
266.430406	11724.839292	27.884903
266.890647	11747.592400	27.889920
266.922509	11779.929060	27.894938
267.388660	11791.172997	27.899956
267.422104	11827.981079	27.904973
267.657644	11845.175651	27.909991
268.442579	11865.609546	27.915008
268.666127	11894.585484	27.920026
269.285830	11909.933842	27.925044
269.359789	11924.976896	27.930061
269.382974	11955.443500	27.935079
269.545139	11972.150069	27.940096
269.929665	11988.065191	27.945114
270.299123	12019.940833	27.950132
270.732717	12030.206333	27.955149
270.915222	12050.444561	27.960167
271.477444	12061.040198	27.965184
271.364637	12084.925228	27.970202
271.884278	12094.860639	27.975220
272.434642	12110.806783	27.980237
272.533991	12133.390805	27.985255
272.706690	12150.436947	27.990272
272.805643	12166.271798	27.995290
272.909698	12183.483729	28.000308
273.367690	12200.246441	28.005325
273.225194	12227.895306	28.010343
273.678720	12253.662892	28.015360
273.715883	12280.687354	28.020378
274.088405	12302.982255	28.025396
274.689306	12329.596168	28.030413
274.966981	12361.885506	28.035431
275.095003	12377.133553	28.040448
275.341502	12402.023267	28.045466
275.728656	12417.812328	28.050484
276.257747	12432.461589	28.055501
276.269244	12455.719209	28.060519
276.713814	12475.738199	28.065536
276.805873	12493.555927	28.070554
277.122287	12525.147468	28.075572
277.512342	12543.895307	28.080589
277.550471	12573.611371	28.085607
278.207228	12580.158761	28.090624
278.717269	12599.559660	28.095642
278.792317	12611.521125	28.100660
279.101294	12633.778924	28.105677
279.121319	12646.512140	28.110695
279.820232	12664.763172	28.115712
279.888208	12685.682124	28.120730
280.114490	12707.665334	28.125748
280.418132	12714.685527	28.130765
280.435063	12741.532898	28.135783
280.599943	12748.550819	28.140800
280.849180	12777.293260	28.145818
281.061456	12793.021765	28.150836
281.170719	12822.001708	28.155853
281.612102	12856.775888	28.160871
281.933557	12866.366348	28.165888
282.025638	12898.054771	28.170906
282.110219	12913.148991	28.175924
282.507064	12944.312862	28.180941
282.553733	12983.618129	28.185959
283.155944	12997.112635	28.190976
283.485216	13026.497800	28.195994
283.597347	13063.597451	28.201012
284.039752	13082.135574	28.206029
284.406206	13120.370415	28.211047
284.750214	13139.575640	28.216064
285.106443	13158.637053	28.221082
285.401898	13173.602132	28.226100
285.999372	13195.408076	28.231117
285.837120	13215.590481	28.236135
286.433224	13238.835371	28.241152
286.331146	13277.445807	28.246170
286.596837	13299.486342	28.251188
287.261303	13326.041763	28.256205
287.194415	13352.075143	28.261223
287.242370	13373.617567	28.266240
287.953193	13397.043855	28.271258
288.400937	13432.752654	28.276276
288.655225	13447.311936	28.281293
288.628953	13482.582304	28.286311
289.160281	13502.215564	28.291328
289.981231	13527.193322	28.296346
290.023502	13553.675423	28.301364
290.159218	13579.812790	28.306381
290.017231	13605.392551	28.311399
290.706440	13626.596153	28.316416
290.682800	13650.208755	28.321434
291.191660	13682.964429	28.326452
291.570395	13709.328165	28.331469
291.417574	13736.304503	28.336487
291.781351	13753.539017	28.341504
291.845525	13795.727081	28.346522
292.274787	13817.115701	28.351540
292.962625	13856.548802	28.356557
293.470048	13878.230298	28.361575
293.762557	13897.202256	28.366592
294.214518	13925.429469	28.371610
294.273750	13938.039036	28.376628
294.714962	13971.370613	28.381645
295.169132	13986.989404	28.386663
294.751506	14009.027183	28.391680
295.401215	14031.151823	28.396698
295.739769	14060.891894	28.401716
296.026373	14093.131998	28.406733
296.172093	14115.784402	28.411751
296.367672	14145.177926	28.416768
297.026774	14158.192830	28.421786
297.706128	14173.440520	28.426804
298.003677	14187.025752	28.431821
297.976951	14214.675424	28.436839
298.237159	14241.538665	28.441856
298.542584	14259.648499	28.446874
298.874571	14297.912299	28.451892
299.349049	14312.497440	28.456909
299.250522	14330.379404	28.461927
299.457799	14344.770763	28.466944
299.582210	14362.485135	28.471962
299.721841	14398.042101	28.476980
299.816458	14423.030929	28.481997
300.209480	14449.989187	28.487015
300.733801	14476.941557	28.492032
300.908500	14505.225039	28.497050
300.988885	14532.124771	28.502068
301.513592	14564.726747	28.507085
301.809378	14587.545699	28.512103
302.004279	14632.517833	28.517120
302.441374	14650.070548	28.522138
302.739340	14682.530568	28.527156
303.346967	14716.852633	28.532173
303.535996	14729.980327	28.537191
303.829613	14762.003125	28.542208
304.236872	14785.142756	28.547226
304.333236	14826.343234	28.552244
304.713768	14842.044355	28.557261
304.980961	14873.520170	28.562279
305.204875	14895.951146	28.567296
305.451194	14922.945455	28.572314
305.854606	14958.151186	28.577332
306.430717	14981.602023	28.582349
306.721788	15016.690911	28.587367
306.846988	15037.852435	28.592384
307.106481	15063.744804	28.597402
307.489398	15101.887037	28.602420
307.826090	15124.740957	28.607437
308.421476	15149.837281	28.612455
308.517157	15189.841078	28.617472
308.894827	15208.934453	28.622490
308.778762	15237.082856	28.627508
309.441103	15265.400564	28.632525
309.671460	15297.893466	28.637543
309.981728	15326.756415	28.642560
310.421957	15345.664684	28.647578
310.573872	15391.389864	28.652596
311.002844	15412.177041	28.657613
311.132924	15444.804999	28.662631
311.502109	15476.124866	28.667648
311.650441	15499.316167	28.672666
311.968739	15534.234616	28.677684
312.920934	15551.648048	28.682701
313.128000	15595.947885	28.687719
313.221348	15620.795343	28.692736
313.869477	15642.391335	28.697754
313.799429	15677.512933	28.702772
314.244749	15693.358619	28.707789
314.694749	15721.770512	28.712807
314.555641	15754.624799	28.717824
315.190326	15783.174919	28.722842
315.316076	15809.746182	28.727860
315.964527	15836.300479	28.732877
316.096851	15866.653159	28.737895
316.261543	15895.585290	28.742912
316.716274	15916.357822	28.747930
316.893414	15957.111250	28.752948
317.365787	15986.311067	28.757965
317.833554	16006.033507	28.762983
318.027151	16041.668665	28.768000
318.464724	16055.846975	28.773018
318.657781	16092.142687	28.778036
319.158836	16114.806933	28.783053
319.449965	16161.671224	28.788071
319.721357	16178.354622	28.793088
320.069500	16200.038736	28.798106
319.989717	16230.253766	28.803124
320.248241	16256.208074	28.808141
320.782007	16293.079938	28.813159
320.749595	16318.795568	28.818176
321.289703	16350.534895	28.823194
321.230448	16390.236248	28.828212
321.470339	16409.588622	28.833229
321.951370	16444.389141	28.838247
322.221980	16472.811485	28.843264
322.739904	16504.132389	28.848282
322.822511	16547.821780	28.853300
323.311017	16584.566235	28.858317
323.693141	16614.223382	28.863335
323.880300	16644.923061	28.868352
324.710933	16669.242100	28.873370
324.866166	16704.210471	28.878388
325.424481	16718.612127	28.883405
325.261349	16749.502261	28.888423
325.895067	16781.340436	28.893440
326.512107	16806.490894	28.898458
326.965865	16840.926377	28.903476
327.096360	16864.798705	28.908493
327.718453	16888.372351	28.913511
327.895144	16912.566523	28.918528
328.399397	16931.867959	28.923546
328.262906	16968.093961	28.928564
328.924613	16990.783316	28.933581
329.486903	17021.396507	28.938599
329.118685	17044.836095	28.943616
329.572685	17071.725561	28.948634
329.946384	17105.062082	28.953652
330.687510	17116.101957	28.958669
330.879940	17156.247451	28.963687
331.079882	17180.378282	28.968704
331.349638	17203.725309	28.973722
331.447535	17228.412107	28.978740
331.825852	17267.862033	28.983757
332.045351	17292.886623	28.988775
332.220928	17329.963420	28.993792
332.912107	17367.952826	28.998810
333.433129	17395.752222	29.003828
333.379380	17427.744626	29.008845
334.179594	17460.990917	29.013863
334.010309	17490.483826	29.018880
334.336194	17525.484068	29.023898
334.761776	17568.925641	29.028916
334.988937	17594.972358	29.033933
335.482313	17626.154450	29.038951
335.652898	17665.048579	29.043968
336.006440	17694.427109	29.048986
336.578244	17738.631488	29.054004
336.906127	17765.977951	29.059021
337.649156	17797.836291	29.064039
337.654605	17817.805940	29.069056
338.332172	17850.564169	29.074074
338.398059	17880.126104	29.079092
338.848349	17902.928880	29.084109
339.355294	17930.190868	29.089127
339.562708	17960.916449	29.094144
339.750353	17979.402931	29.099162
340.051279	18021.072563	29.104180
340.269439	18052.458548	29.109197
340.875649	18076.202027	29.114215
340.898175	18110.572699	29.119232
341.537411	18139.099375	29.124250
341.599532	18172.932448	29.129268
342.167029	18209.948053	29.134285
342.526250	18239.057079	29.139303
342.658810	18269.570198	29.144320
343.120834	18300.024218	29.149338
343.401405	18317.565745	29.154356
343.724778	18351.926625	29.159373
343.865300	18366.862165	29.164391
344.268576	18409.937642	29.169408
344.675767	18433.496991	29.174426
345.050782	18458.341608	29.179444
345.325634	18489.348638	29.184461
345.605315	18525.186168	29.189479
345.939684	18561.274824	29.194496
346.680231	18581.292616	29.199514
346.793857	18618.444014	29.204532
347.027700	18640.946246	29.209549
347.582073	18682.055504	29.214567
347.662320	18713.041507	29.219584
348.064918	18734.303829	29.224602
347.981248	18775.026923	29.229620
348.326010	18808.002814	29.234637
349.169165	18840.712010	29.239655
349.446575	18883.197911	29.244672
349.872302	18912.576140	29.249690
350.229585	18949.282918	29.254708
350.235496	18993.328779	29.259725
350.747716	19019.685318	29.264743
350.857859	19049.811076	29.269760
351.550021	19086.595247	29.274778
352.340759	19117.234491	29.279796
352.258824	19154.846578	29.284813
352.935160	19179.975105	29.289831
352.870701	19219.398799	29.294848
353.662336	19250.127992	29.299866
354.176795	19285.416073	29.304884
353.872292	19312.612622	29.309901
354.079919	19351.996411	29.314919
354.658610	19392.260071	29.319936
355.842997	19423.471695	29.324954
355.788099	19459.117453	29.329972
356.340039	19479.664043	29.334989
356.991680	19509.948669	29.340007
356.791979	19532.908362	29.345024
357.426973	19571.794880	29.350042
357.625538	19602.219152	29.355060
357.513584	19631.925510	29.360077
358.040152	19669.826024	29.365095
358.539466	19702.669392	29.370112
359.114078	19737.310066	29.375130
358.890600	19776.471296	29.380148
358.928055	19814.763487	29.385165
359.156541	19847.328722	29.390183
359.375393	19903.123731	29.395200
360.052072	19944.720357	29.400218
360.149603	19983.097594	29.405236
360.730279	20031.258662	29.410253
361.212370	20078.061526	29.415271
361.204949	20120.731638	29.420288
362.387747	20171.528718	29.425306
362.937848	20206.885383	29.430324
363.390622	20243.133116	29.435341
363.964837	20275.684638	29.440359
364.381838	20307.157119	29.445376
364.806218	20327.929192	29.450394
365.114637	20348.731482	29.455412
365.568470	20380.827014	29.460429
366.167733	20406.288571	29.465447
366.194874	20438.312823	29.470464
366.281062	20466.390997	29.475482
366.734533	20488.488985	29.480500
366.999984	20525.487137	29.485517
367.676978	20548.913486	29.490535
367.849138	20587.716463	29.495552
368.076764	20604.821441	29.500570
368.642719	20633.451224	29.505588
368.634301	20664.204849	29.510605
369.225939	20688.930313	29.515623
369.517846	20716.062150	29.520640
369.920584	20742.311815	29.525658
370.384113	20783.073959	29.530676
370.310579	20817.538610	29.535693
370.564254	20842.975948	29.540711
370.733050	20869.778393	29.545728
371.295108	20912.638641	29.550746
371.485853	20944.868579	29.555764
371.422281	20995.410580	29.560781
372.025338	21025.069087	29.565799
372.700476	21076.756806	29.570816
373.012087	21122.958586	29.575834
373.420222	21157.987582	29.580852
373.761365	21207.243146	29.585869
374.359327	21237.281235	29.590887
374.811323	21282.591603	29.595904
374.966641	21315.753525	29.600922
375.583360	21350.150964	29.605940
375.871999	21398.236520	29.610957
376.817935	21428.739301	29.615975
376.829564	21461.092837	29.620992
377.156042	21495.331994	29.626010
377.718651	21524.124664	29.631028
378.113890	21565.604711	29.636045
378.672012	21597.363737	29.641063
378.971807	21633.512058	29.646080
379.368743	21661.235050	29.651098
379.940486	21694.582756	29.656116
380.087502	21728.662848	29.661133
380.577112	21756.493661	29.666151
381.170172	21793.038472	29.671168
381.525905	21823.890148	29.676186
381.913786	21854.312472	29.681204
382.125875	21894.830347	29.686221
382.638105	21910.937392	29.691239
382.923727	21950.027484	29.696256
383.243328	21988.790429	29.701274
383.690868	22014.993698	29.706292
383.911163	22039.404124	29.711309
384.564112	22069.954900	29.716327
384.964981	22103.571290	29.721344
384.899135	22145.884132	29.726362
385.238382	22176.628817	29.731380
385.441807	22221.967020	29.736397
386.226870	22255.863949	29.741415
386.578754	22292.886412	29.746432
386.599620	22325.634239	29.751450
387.325841	22362.205591	29.756468
387.615597	22402.399687	29.761485
388.025578	22439.327737	29.766503
388.387476	22476.369445	29.771520
388.843964	22517.013992	29.776538
389.378411	22551.608800	29.781556
389.660327	22588.179938	29.786573
390.298313	22624.012800	29.791591
390.716626	22651.683444	29.796608
390.545379	22695.260629	29.801626
391.170966	22715.034364	29.806644
391.650278	22758.838497	29.811661
392.078558	22788.199475	29.816679
392.407419	22827.509925	29.821696
392.157197	22861.249574	29.826714
393.071087	22892.490316	29.831732
393.556662	22930.330885	29.836749
394.129535	22959.007648	29.841767
394.741993	22996.775376	29.846784
394.937592	23019.937841	29.851802
395.566598	23048.305913	29.856820
395.981566	23076.748808	29.861837
396.349631	23099.359431	29.866855
396.878720	23135.395844	29.871872
396.959183	23156.668138	29.876890
397.420076	23184.280592	29.881908
397.685855	23213.029015	29.886925
398.104410	23240.523995	29.891943
398.367762	23271.193345	29.896960
398.310276	23305.151161	29.901978
399.068230	23337.850143	29.906996
399.475775	23376.114549	29.912013
399.818599	23408.043430	29.917031
400.017165	23437.113951	29.922048
400.461196	23489.809073	29.927066
400.922730	23513.587357	29.932084
400.991916	23564.100944	29.937101
401.226871	23598.152945	29.942119
401.880069	23649.699258	29.947136
402.112703	23700.859522	29.952154
402.631927	23729.169615	29.957172
403.007764	23787.352984	29.962189
403.590194	23837.254389	29.967207
403.744859	23869.853812	29.972224
404.093687	23928.193496	29.977242
404.479435	23960.494753	29.982260
404.940424	24011.019058	29.987277
405.433844	24047.582068	29.992295
405.712303	24096.310867	29.997312
406.042793	24145.989900	30.002330
406.488092	24193.592396	30.007348
406.975941	24248.676213	30.012365
407.182084	24289.784232	30.017383
407.989274	24343.081121	30.022400
408.487642	24391.507961	30.027418
409.322700	24421.616640	30.032436
409.610114	24475.655763	30.037453
409.828612	24507.962039	30.042471
410.719848	24548.577500	30.047488
411.204805	24596.551437	30.052506
411.624371	24619.530871	30.057524
412.003158	24656.010058	30.062541
412.194406	24695.713405	30.067559
412.397528	24734.533427	30.072576
412.739464	24772.486993	30.077594
413.564519	24803.875251	30.082612
413.869688	24857.887426	30.087629
414.266032	24892.558722	30.092647
414.879214	24933.344031	30.097664
414.878824	24968.569845	30.102682
415.701155	25005.220927	30.107700
415.795246	25040.877537	30.112717
416.286367	25078.576920	30.117735
416.601938	25113.640459	30.122752
416.821395	25170.890926	30.127770
417.426486	25205.564645	30.132788
417.668756	25243.601955	30.137805
418.157627	25289.677047	30.142823
418.237987	25320.558518	30.147840
418.551057	25372.688203	30.152858
419.258009	25415.491806	30.157876
419.823669	25473.785206	30.162893
419.913360	25525.387722	30.167911
420.798763	25559.577475	30.172928
420.768366	25608.128239	30.177946
421.186314	25636.634860	30.182964
421.653232	25683.529914	30.187981
421.901809	25726.253899	30.192999
422.431189	25763.738745	30.198016
422.471195	25812.592270	30.203034
423.492865	25851.408929	30.208052
423.907712	25897.737587	30.213069
424.057448	25938.158734	30.218087
424.420095	25991.624108	30.223104
424.660135	26029.220410	30.228122
425.851377	26082.328419	30.233140
426.177018	26122.310932	30.238157
426.401722	26153.406610	30.243175
427.009400	26200.685114	30.248192
427.273041	26242.346593	30.253210
427.673211	26284.383022	30.258228
428.513913	26321.123790	30.263245
428.680568	26372.377095	30.268263
429.212806	26403.327806	30.273280
429.676965	26445.164819	30.278298
430.351258	26478.681638	30.283316
430.923949	26519.986803	30.288333
431.094058	26555.936801	30.293351
431.676282	26599.114073	30.298368
431.856242	26640.768266	30.303386
432.181947	26668.839241	30.308404
432.514372	26720.473075	30.313421
433.057687	26773.198228	30.318439
433.463428	26819.770595	30.323456
433.763530	26870.968650	30.328474
434.166825	26912.614997	30.333492
434.697257	26948.569379	30.338509
434.888601	27001.444843	30.343527
435.596035	27044.429077	30.348544
435.668960	27096.346619	30.353562
436.134524	27144.559591	30.358580
437.210269	27186.010360	30.363597
437.310627	27240.980169	30.368615
438.078496	27284.365060	30.373632
438.143077	27334.054708	30.378650
438.686801	27377.076281	30.383668
439.292876	27418.860684	30.388685
439.235883	27480.843765	30.393703
439.920165	27530.150890	30.398720
440.086312	27570.841277	30.403738
440.688634	27622.638261	30.408756
441.306977	27674.792336	30.413773
441.662881	27721.107267	30.418791
442.112406	27773.018261	30.423808
442.324020	27822.063641	30.428826
442.952306	27869.718696	30.433844
443.270231	27918.409283	30.438861
443.922203	27969.681808	30.443879
444.450415	28024.242776	30.448896
444.878061	28070.455320	30.453914
444.775008	28118.585150	30.458932
445.395503	28171.342846	30.463949
445.995720	28224.921023	30.468967
446.728786	28265.128265	30.473984
447.216284	28324.617674	30.479002
447.559052	28378.702544	30.484020
448.157223	28405.967993	30.489037
448.356717	28455.799457	30.494055
448.897986	28503.234058	30.499072
449.240119	28554.127350	30.504090
449.462801	28608.169686	30.509108
450.053081	28647.401460	30.514125
450.600998	28698.687030	30.519143
451.346347	28734.070235	30.524160
451.592304	28784.999019	30.529178
452.066838	28818.253727	30.534196
452.989592	28856.415328	30.539213
452.938499	28902.579844	30.544231
453.787007	28932.653244	30.549248
453.739198	28974.480030	30.554266
454.249536	29013.312604	30.559284
454.829022	29062.688737	30.564301
454.970516	29095.976910	30.569319
456.059963	29136.373362	30.574336
456.442077	29183.331399	30.579354
456.682319	29237.174063	30.584372
457.232336	29266.439323	30.589389
457.209801	29312.675920	30.594407
457.803125	29369.889644	30.599424
458.319240	29417.901878	30.604442
458.606152	29467.731275	30.609460
459.347741	29514.785402	30.614477
459.246498	29571.038813	30.619495
460.162776	29619.234715	30.624512
460.385909	29675.179360	30.629530
460.695812	29731.283355	30.634548
461.760466	29783.073534	30.639565
461.788069	29840.830211	30.644583
462.355737	29885.444003	30.649600
462.788439	29933.029790	30.654618
463.405815	29986.462314	30.659636
464.074802	30029.996623	30.664653
464.293490	30085.167275	30.669671
465.066518	30125.892758	30.674688
466.056248	30156.575894	30.679706
466.202820	30201.379931	30.684724
466.547412	30238.532784	30.689741
467.208938	30290.671834	30.694759
467.792753	30331.482684	30.699776
468.169827	30378.924298	30.704794
468.173630	30435.317727	30.709812
469.035737	30462.984481	30.714829
468.935743	30518.458367	30.719847
469.555511	30572.302410	30.724864
470.158962	30625.922172	30.729882
470.578079	30676.849977	30.734900
470.878256	30725.810064	30.739917
471.319691	30785.791884	30.744935
472.012286	30823.677198	30.749952
472.580045	30886.124480	30.754970
473.156718	30928.669900	30.759988
473.969212	30974.444871	30.765005
474.153387	31030.267795	30.770023
474.754970	31076.986467	30.775040
475.342315	31115.691132	30.780058
475.703363	31169.049736	30.785076
476.350927	31213.609561	30.790093
476.430482	31250.243624	30.795111
476.824851	31301.745215	30.800128
477.491337	31346.595659	30.805146
477.833638	31403.251784	30.810164
478.666702	31436.452277	30.815181
478.688565	31480.201210	30.820199
479.385197	31519.696377	30.825216
479.695853	31578.560434	30.830234
479.962590	31634.226517	30.835252
480.477354	31667.921718	30.840269
480.851612	31734.395004	30.845287
481.204964	31782.317589	30.850304
481.789361	31846.800507	30.855322
481.964554	31895.932793	30.860340
482.537134	31941.854041	30.865357
482.744958	31999.291503	30.870375
483.415176	32054.362229	30.875392
483.787904	32111.807525	30.880410
483.977748	32160.499582	30.885428
484.716481	32218.143483	30.890445
484.854448	32275.855256	30.895463
485.411974	32343.161904	30.900480
486.063919	32404.660477	30.905498
485.791411	32469.407114	30.910516
487.063595	32518.306303	30.915533
487.772282	32582.143523	30.920551
488.588681	32631.235052	30.925568
489.182322	32687.673960	30.930586
489.596401	32741.195803	30.935604
490.364098	32786.667394	30.940621
490.737379	32835.782204	30.945639
491.211807	32885.057134	30.950656
491.934910	32940.197623	30.955674
492.392530	32983.269365	30.960692
493.327086	33019.261055	30.965709
493.709563	33075.568860	30.970727
494.027439	33126.258612	30.975744
494.195976	33176.540912	30.980762
494.625721	33222.025276	30.985780
495.126661	33279.298595	30.990797
495.421901	33331.816406	30.995815
496.569567	33372.885125	31.000832
497.620275	33412.256646	31.005850
497.945349	33462.450798	31.010868
498.631406	33498.421409	31.015885
498.696316	33545.907367	31.020903
499.443376	33588.958020	31.025920
500.232362	33629.281983	31.030938
500.040303	33675.611718	31.035956
500.612525	33714.337227	31.040973
500.839397	33767.432426	31.045991
501.083525	33823.178572	31.051008
501.734004	33867.160904	31.056026
502.182346	33937.612306	31.061044
502.944587	33984.725518	31.066061
503.798191	34037.875775	31.071079
503.931250	34078.097694	31.076096
504.706486	34117.532068	31.081114
505.194018	34173.573583	31.086132
506.213206	34217.751473	31.091149
506.137831	34255.900411	31.096167
506.409885	34319.102905	31.101184
507.013892	34364.258501	31.106202
507.286970	34417.912837	31.111220
507.952564	34466.390669	31.116237
508.232648	34530.072217	31.121255
508.798525	34587.414771	31.126272
509.448640	34639.196257	31.131290
509.276788	34688.813308	31.136308
509.968386	34762.698845	31.141325
510.396734	34824.444721	31.146343
510.745387	34878.952576	31.151360
511.391510	34945.594988	31.156378
511.824062	35014.737410	31.161396
512.205718	35078.442009	31.166413
512.691928	35139.882798	31.171431
513.201737	35216.125900	31.176448
513.945276	35274.697246	31.181466
514.138737	35349.330171	31.186484
514.836029	35406.142448	31.191501
515.310844	35469.981371	31.196519
516.103231	35536.952111	31.201536
516.812230	35577.959556	31.206554
516.876103	35639.351910	31.211572
517.482077	35687.669355	31.216589
518.354694	35746.852066	31.221607
518.955272	35799.673860	31.226624
519.645388	35852.512578	31.231642
520.250869	35903.352091	31.236660
520.404869	35958.589651	31.241677
520.841824	36015.980186	31.246695
521.321543	36067.298518	31.251712
521.996509	36126.786528	31.256730
522.271922	36186.706799	31.261748
523.039697	36239.341332	31.266765
523.845364	36294.090442	31.271783
524.233614	36336.171924	31.276800
524.905735	36400.309781	31.281818
525.365928	36441.391864	31.286836
526.288881	36488.055970	31.291853
526.797255	36551.183154	31.296871
527.059317	36608.465619	31.301888
527.409311	36656.360899	31.306906
527.684317	36704.432797	31.311924
528.567638	36767.003342	31.316941
528.971860	36823.464580	31.321959
529.082107	36889.486370	31.326976
530.047091	36962.903494	31.331994
530.147552	37018.475061	31.337012
531.207499	37080.184367	31.342029
531.218186	37146.491797	31.347047
531.611930	37206.358055	31.352064
532.527637	37263.256921	31.357082
532.834415	37339.687771	31.362100
533.284728	37386.334447	31.367117
533.835960	37446.326978	31.372135
534.572617	37529.075326	31.377152
535.192521	37587.112893	31.382170
535.546537	37651.345631	31.387188
536.548100	37709.724524	31.392205
537.239403	37768.243221	31.397223
537.417368	37826.083133	31.402240
538.355970	37892.827068	31.407258
538.783190	37952.724993	31.412276
539.362699	37994.545218	31.417293
539.825394	38062.624504	31.422311
540.389065	38123.166391	31.427328
541.011164	38172.153799	31.432346
541.604227	38231.854829	31.437364
541.837599	38304.003259	31.442381
542.390983	38361.262116	31.447399
542.512162	38427.382411	31.452416
543.368227	38484.171896	31.457434
543.539518	38560.137928	31.462452
544.558880	38622.670358	31.467469
545.181273	38691.079125	31.472487
545.339233	38753.962595	31.477504
545.949992	38813.599497	31.482522
546.698091	38888.862487	31.487540
547.293083	38950.475087	31.492557
547.617908	39011.933676	31.497575
548.019690	39085.610276	31.502592
549.033035	39143.221730	31.507610
549.517087	39216.433927	31.512628
550.392855	39276.233738	31.517645
550.541716	39330.829121	31.522663
551.036051	39389.748572	31.527680
551.606511	39456.230824	31.532698
552.059364	39520.876817	31.537716
552.609682	39575.955831	31.542733
553.150889	39642.601414	31.547751
553.512554	39699.470053	31.552768
554.186148	39751.650629	31.557786
554.617485	39820.742266	31.562804
555.269741	39885.896364	31.567821
555.894460	39943.965942	31.572839
556.492200	40000.029520	31.577856
556.929239	40066.412938	31.582874
557.022058	40129.596000	31.587892
557.697337	40194.608516	31.592909
558.362344	40264.468137	31.597927
558.440118	40341.965847	31.602944
559.347319	40415.990477	31.607962
559.609779	40494.525225	31.612980
560.167797	40565.985080	31.617997
560.763228	40630.213736	31.623015
561.322493	40712.753384	31.628032
562.638842	40768.467049	31.633050
563.271546	40843.132182	31.638068
564.056447	40900.212437	31.643085
564.754910	40960.552118	31.648103
565.131999	41028.823947	31.653120
566.037379	41086.462542	31.658138
565.988261	41154.577958	31.663156
566.773084	41221.078585	31.668173
567.587175	41276.529527	31.673191
568.301173	41335.122254	31.678208
568.869955	41390.481479	31.683226
569.454687	41453.685722	31.688244
569.736528	41513.767743	31.693261
570.421789	41574.304184	31.698279
570.890817	41644.618127	31.703296
571.464687	41710.047367	31.708314
571.989877	41769.534450	31.713332
572.469065	41837.426244	31.718349
572.897776	41901.295458	31.723367
573.292300	41973.270786	31.728384
574.241610	42051.007425	31.733402
574.432622	42115.721619	31.738420
574.843554	42183.490222	31.743437
575.581799	42260.934301	31.748455
575.990508	42342.158185	31.753472
577.078985	42403.846139	31.758490
577.545814	42485.525110	31.763508
577.830821	42552.839185	31.768525
578.683926	42631.212908	31.773543
579.003451	42693.606543	31.778560
579.680027	42767.044220	31.783578
580.258991	42843.854107	31.788596
580.913483	42913.147834	31.793613
581.461292	42986.430864	31.798631
581.858857	43071.921661	31.803648
582.827879	43143.879281	31.808666
583.208768	43227.593025	31.813684
583.532174	43298.366674	31.818701
584.515128	43358.515700	31.823719
584.859881	43434.722695	31.828736
585.917982	43505.233727	31.833754
586.450497	43577.707112	31.838772
587.013038	43638.943051	31.843789
587.996165	43710.707967	31.848807
588.565322	43769.291315	31.853824
589.089202	43833.094663	31.858842
589.388591	43902.021379	31.863860
589.877358	43967.008580	31.868877
590.816560	44037.645461	31.873895
591.274034	44096.911283	31.878912
591.826732	44170.526529	31.883930
592.372111	44224.341653	31.888948
592.593285	44293.816297	31.893965
593.285618	44347.793779	31.898983
593.789299	44419.495392	31.904000
594.278065	44493.150889	31.909018
594.701582	44562.583645	31.914036
594.961202	44646.004934	31.919053
595.657719	44706.625551	31.924071
596.234088	44794.342691	31.929088
596.617686	44858.958879	31.934106
597.364049	44954.516571	31.939124
597.559072	45033.533243	31.944141
598.595238	45115.960126	31.949159
598.915544	45208.451133	31.954176
599.127526	45293.790200	31.959194
599.962934	45380.270683	31.964212
600.688273	45464.007060	31.969229
601.427860	45540.249025	31.974247
601.903304	45633.805804	31.979264
602.985401	45721.601640	31.984282
603.566345	45790.744582	31.989300
603.961295	45880.451218	31.994317
604.703701	45961.891556	31.999335
605.009042	46049.223618	32.004352
605.879217	46132.061290	32.009370
607.014594	46214.890260	32.014388
607.282636	46309.119316	32.019405
608.139549	46388.856493	32.024423
608.182756	46475.406562	32.029440
608.579491	46554.102679	32.034458
609.613676	46648.768943	32.039476
609.886102	46739.886085	32.044493
610.733549	46829.345693	32.049511
610.993616	46912.458079	32.054528
611.992191	47010.355952	32.059546
612.516779	47105.547586	32.064564
612.937361	47190.074565	32.069581
613.950764	47282.335007	32.074599
614.451600	47368.860962	32.079616
615.103420	47453.954047	32.084634
616.006369	47537.970314	32.089652
616.272091	47629.819131	32.094669
617.282039	47719.022451	32.099687
617.492658	47795.427236	32.104704
618.713818	47882.891265	32.109722
619.456670	47952.719588	32.114740
620.635776	48024.677094	32.119757
621.689482	48093.570419	32.124775
622.520876	48163.107011	32.129792
623.412080	48222.396336	32.134810
623.670383	48288.364970	32.139828
624.293962	48352.909320	32.144845
625.122357	48415.001151	32.149863
625.271935	48488.011491	32.154880
625.944571	48550.281067	32.159898
626.517057	48612.201074	32.164916
627.157415	48686.722696	32.169933
627.693593	48748.585985	32.174951
628.089414	48825.548545	32.179968
628.858389	48885.482242	32.184986
629.458110	48950.983102	32.190004
629.633350	49034.270390	32.195021
630.350512	49110.438913	32.200039
630.514329	49183.819054	32.205056
631.143730	49262.958547	32.210074
631.746793	49345.826004	32.215092
632.168240	49435.851460	32.220109
632.724813	49509.430104	32.225127
633.271969	49587.352895	32.230144
633.947159	49675.426959	32.235162
634.720598	49746.734798	32.240180
635.096241	49833.324240	32.245197
635.864166	49907.071629	32.250215
636.427821	50002.441875	32.255232
636.972658	50086.942276	32.260250
637.682180	50166.574425	32.265268
638.081711	50255.088296	32.270285
638.859714	50334.403493	32.275303
639.216387	50423.332622	32.280320
639.933168	50508.314953	32.285338
640.708040	50601.834182	32.290356
641.372406	50696.433280	32.295373
642.025357	50787.036398	32.300391
642.623835	50887.644820	32.305408
642.730825	50976.216648	32.310426
643.615204	51061.236914	32.315444
644.277535	51163.901756	32.320461
644.954340	51257.771997	32.325479
645.756148	51351.669426	32.330496
646.521295	51444.439522	32.335514
647.599253	51544.425799	32.340532
647.781249	51632.568195	32.345549
648.787160	51724.999834	32.350567
649.526283	51808.224997	32.355584
650.153092	51909.187821	32.360602
651.277760	51990.322390	32.365620
651.693364	52076.318396	32.370637
652.402459	52157.184344	32.375655
653.401573	52253.555086	32.380672
653.772753	52333.372110	32.385690
654.665997	52405.535463	32.390708
655.253718	52492.897798	32.395725
656.020379	52574.318201	32.400743
656.791809	52665.011652	32.405760
656.804908	52755.110615	32.410778
658.027785	52835.477617	32.415796
658.233062	52928.723175	32.420813
659.091867	53013.074011	32.425831
659.858899	53092.039134	32.430848
660.561688	53171.627962	32.435866
661.145657	53260.226240	32.440884
661.478925	53353.477968	32.445901
661.867326	53428.211212	32.450919
663.353493	53528.797337	32.455936
663.847904	53612.503410	32.460954
664.833199	53691.813970	32.465972
665.005414	53779.920365	32.470989
666.385273	53869.792455	32.476007
666.904397	53946.818302	32.481024
667.050773	54030.040340	32.486042
667.731038	54110.818111	32.491060
668.090320	54206.476617	32.496077
668.709057	54296.729079	32.501095
669.371204	54387.833989	32.506112
669.921850	54491.422532	32.511130
671.006588	54579.463962	32.516148
671.783633	54660.967199	32.521165
672.587619	54747.457363	32.526183
673.733105	54829.645952	32.531200
674.142234	54919.626334	32.536218
675.147481	54999.393798	32.541236
676.063357	55073.168047	32.546253
676.645424	55153.530410	32.551271
677.175753	55222.921093	32.556288
677.875533	55306.549964	32.561306
678.440090	55367.008243	32.566324
678.664420	55438.162391	32.571341
679.276881	55518.931901	32.576359
679.922603	55596.556181	32.581376
680.347401	55676.276944	32.586394
681.295296	55755.235606	32.591412
681.739079	55842.232352	32.596429
682.149017	55921.893383	32.601447
683.248598	56021.368372	32.606464
683.444999	56106.663323	32.611482
684.260168	56189.436571	32.616500
684.655363	56282.957387	32.621517
685.061562	56370.379676	32.626535
685.823897	56474.278586	32.631552
686.091512	56583.011149	32.636570
686.651568	56672.917757	32.641588
687.398938	56791.656388	32.646605
688.167029	56895.341735	32.651623
689.000715	56990.619518	32.656640
689.502504	57115.813918	32.661658
690.265934	57221.131922	32.666676
690.652753	57323.846232	32.671693
691.415691	57446.737537	32.676711
692.427192	57544.269645	32.681728
692.855290	57667.255524	32.686746
693.764705	57774.846048	32.691764
694.616564	57886.844526	32.696781
695.112803	57996.772925	32.701799
696.082030	58107.299936	32.706816
696.472594	58217.979993	32.711834
697.641074	58317.012819	32.716852
698.751715	58419.764910	32.721869
700.209733	58515.484016	32.726887
701.682435	58584.490746	32.731904
702.313938	58680.922170	32.736922
703.187680	58758.875057	32.741940
703.961470	58842.354990	32.746957
704.468803	58916.944064	32.751975
705.478431	58991.494701	32.756992
705.560619	59073.693287	32.762010
706.316743	59151.761918	32.767028
706.943431	59244.626524	32.772045
707.320014	59335.529666	32.777063
707.990946	59419.028992	32.782080
708.606291	59515.315444	32.787098
708.980364	59602.340167	32.792116
709.426126	59701.044218	32.797133
710.188534	59801.017212	32.802151
710.982018	59909.175530	32.807168
711.100715	59995.814411	32.812186
711.771855	60116.828837	32.817204
712.584361	60223.412155	32.822221
713.066998	60337.545493	32.827239
714.061695	60439.290692	32.832256
714.816070	60545.866357	32.837274
715.876854	60646.653748	32.842292
716.438881	60759.860019	32.847309
716.875791	60881.303218	32.852327
717.735859	60977.056994	32.857344
718.427967	61095.666009	32.862362
718.921144	61201.548856	32.867380
719.529355	61305.991294	32.872397
720.045531	61432.461633	32.877415
721.061458	61541.198679	32.882432
721.458845	61660.712865	32.887450
722.439649	61768.534216	32.892468
723.238613	61887.073340	32.897485
723.449578	61999.415471	32.902503
724.644926	62096.180943	32.907520
725.126706	62219.527099	32.912538
725.915878	62316.878949	32.917556
726.872809	62428.234398	32.922573
727.758723	62531.695574	32.927591
728.506452	62627.779069	32.932608
728.968812	62738.276168	32.937626
729.599522	62848.423728	32.942644
730.617413	62955.404646	32.947661
730.970785	63057.382663	32.952679
731.886941	63169.368295	32.957696
732.645418	63285.887070	32.962714
733.310187	63385.628421	32.967732
734.115488	63495.295561	32.972749
734.818976	63617.608592	32.977767
735.753241	63725.903070	32.982784
736.398978	63841.204787	32.987802
737.423299	63937.710172	32.992820
738.469263	64041.967932	32.997837
738.900503	64166.181158	33.002855
739.742530	64263.508272	33.007872
740.344231	64379.869534	33.012890
740.977591	64485.916942	33.017908
741.232189	64605.655238	33.022925
742.301637	64720.354644	33.027943
743.010039	64841.530067	33.032960
743.577995	64955.687825	33.037978
744.575826	65080.868607	33.042996
745.429320	65191.952753	33.048013
746.166264	65314.927743	33.053031
746.972376	65428.599990	33.058048
747.642813	65542.763032	33.063066
748.359022	65660.642329	33.068084
749.642699	65772.878550	33.073101
750.088422	65896.031509	33.078119
750.947862	65992.706495	33.083136
751.237077	66121.632696	33.088154
752.266347	66243.800048	33.093172
753.275909	66352.095887	33.098189
753.717881	66465.088026	33.103207
754.428260	66584.794111	33.108224
755.625159	66707.296832	33.113242
756.022741	66816.574840	33.118260
756.978450	66933.600014	33.123277
757.663093	67058.035291	33.128295
758.844958	67168.102265	33.133312
759.410447	67281.287049	33.138330
760.065276	67397.555336	33.143348
760.912881	67517.376872	33.148365
761.607351	67640.410567	33.153383
762.445807	67747.667211	33.158400
763.009640	67868.991642	33.163418
763.503963	67978.664352	33.168436
764.619454	68099.955920	33.173453
765.152700	68224.853032	33.178471
766.171655	68343.886044	33.183488
766.782330	68473.898998	33.188506
767.472730	68581.190677	33.193524
768.603745	68704.322901	33.198541
768.773345	68827.222632	33.203559
769.745113	68957.697365	33.208576
770.428386	69070.840744	33.213594
771.357859	69202.759125	33.218612
772.279650	69314.916087	33.223629
772.746808	69443.043067	33.228647
773.426500	69565.319144	33.233664
774.149766	69689.042887	33.238682
775.055024	69809.772074	33.243700
775.976752	69919.175669	33.248717
776.470964	70042.066798	33.253735
777.319544	70147.253889	33.258752
778.318764	70268.589786	33.263770
778.878978	70381.071335	33.268788
779.779275	70495.899929	33.273805
780.457274	70625.598874	33.278823
781.260573	70738.851481	33.283840
782.357827	70846.466836	33.288858
782.976294	70960.775433	33.293876
783.863837	71069.804915	33.298893
784.355541	71191.248855	33.303911
785.285759	71316.882704	33.308928
786.112487	71437.305319	33.313946
786.657012	71558.540293	33.318964
787.445622	71672.944747	33.323981
787.906974	71809.787400	33.328999
789.119953	71927.240398	33.334016
789.932747	72062.237202	33.339034
790.560829	72183.822338	33.344052
791.569636	72302.468246	33.349069
792.189137	72430.335120	33.354087
792.944782	72554.183975	33.359104
793.714352	72692.359835	33.364122
794.483282	72811.478151	33.369140
795.508851	72945.635990	33.374157
796.006927	73074.317166	33.379175
796.923651	73202.879393	33.384192
798.048903	73338.445995	33.389210
798.292397	73463.409056	33.394228
799.578026	73598.811695	33.399245
800.033149	73733.454370	33.404263
801.203895	73857.665854	33.409280
801.811332	73995.541685	33.414298
802.405929	74132.680637	33.419316
803.426903	74259.619390	33.424333
804.086808	74405.204148	33.429351
805.409269	74544.179569	33.434368
806.117857	74664.260316	33.439386
807.091465	74791.677970	33.444404
808.107391	74917.577960	33.449421
808.535062	75048.097465	33.454439
809.356652	75188.045068	33.459456
810.450477	75306.857861	33.464474
811.493018	75436.784886	33.469492
812.151497	75561.185567	33.474509
812.751114	75693.590431	33.479527
813.508192	75821.441960	33.484544
814.608945	75950.641471	33.489562
814.884781	76090.526870	33.494580
816.074036	76206.185627	33.499597
816.861858	76343.021990	33.504615
817.473215	76481.874206	33.509632
818.691347	76610.634494	33.514650
819.406213	76741.097703	33.519668
820.534730	76873.017592	33.524685
820.795492	77001.539810	33.529703
821.568311	77133.336581	33.534720
822.513958	77261.677657	33.539738
823.320599	77402.755007	33.544756
823.842683	77535.689753	33.549773
824.542872	77687.949609	33.554791
825.302438	77820.461045	33.559808
826.446810	77954.636412	33.564826
826.738786	78095.676672	33.569844
827.972023	78231.160939	33.574861
828.517246	78380.440494	33.579879
829.735568	78518.667683	33.584896
830.775574	78635.489683	33.589914
831.466468	78761.889147	33.594932
832.112487	78885.912181	33.599949
833.063600	79014.490220	33.604967
833.953522	79136.159380	33.609984
834.987271	79268.918825	33.615002
835.592748	79388.745099	33.620020
836.762190	79514.873738	33.625037
837.348300	79647.703028	33.630055
837.950011	79776.697374	33.635072
838.771583	79904.663077	33.640090
839.657305	80050.943649	33.645108
840.394971	80177.640707	33.650125
841.098471	80312.984744	33.655143
841.574521	80442.104880	33.660160
842.660102	80591.000047	33.665178
843.229710	80744.542167	33.670196
844.135711	80889.958252	33.675213
844.931594	81036.057659	33.680231
845.551228	81190.530764	33.685248
846.801823	81326.404163	33.690266
847.373844	81477.920309	33.695284
848.542065	81618.142254	33.700301
849.498925	81769.438665	33.705319
850.549660	81915.185389	33.710336
851.383772	82058.166410	33.715354
852.579474	82206.098839	33.720372
853.625488	82332.738123	33.725389
854.547630	82479.768599	33.730407
855.536003	82610.872528	33.735424
856.752769	82741.610542	33.740442
857.433118	82886.501047	33.745460
858.363835	83015.687337	33.750477
858.854994	83155.113280	33.755495
859.630705	83287.407607	33.760512
860.710193	83429.059843	33.765530
861.306744	83566.826046	33.770548
862.313701	83707.359559	33.775565
863.581868	83835.900092	33.780583
864.430447	83981.446704	33.785600
865.342490	84106.764100	33.790618
866.099074	84245.001433	33.795636
866.672166	84385.395643	33.800653
867.884544	84525.805363	33.805671
868.573946	84670.528532	33.810688
869.493238	84806.148429	33.815706
870.359384	84947.339141	33.820724
870.887078	85086.233026	33.825741
871.756452	85231.524727	33.830759
872.343537	85369.594347	33.835776
873.416082	85521.908821	33.840794
874.331275	85665.228008	33.845812
875.338222	85810.000803	33.850829
875.705150	85965.212266	33.855847
876.495741	86117.431694	33.860864
877.402279	86262.268184	33.865882
877.827739	86437.283428	33.870900
878.952241	86569.785796	33.875917
879.257392	86737.717693	33.880935
880.507190	86905.532791	33.885952
881.679008	87063.390054	33.890970
882.552791	87231.206310	33.895988
884.053678	87369.649465	33.901005
884.464134	87521.890226	33.906023
885.519945	87676.202090	33.911040
886.859571	87821.609519	33.916058
887.587343	87969.997937	33.921076
888.755518	88116.460578	33.926093
889.351738	88260.202753	33.931111
890.213485	88398.137412	33.936128
891.095485	88527.843455	33.941146
892.044749	88664.290861	33.946164
892.855451	88795.876853	33.951181
893.935669	88939.037037	33.956199
894.719038	89079.418532	33.961216
895.664427	89204.371910	33.966234
896.401470	89338.301773	33.971252
897.803081	89481.190703	33.976269
898.937214	89615.043915	33.981287
899.192722	89748.815143	33.986304
900.272282	89882.938332	33.991322
901.286675	90027.204415	33.996340
901.968611	90166.969969	34.001357
902.590042	90316.782910	34.006375
903.196871	90459.214112	34.011392
904.201795	90618.901024	34.016410
905.136906	90773.151821	34.021428
905.987039	90926.417761	34.026445
906.515430	91081.465471	34.031463
907.210407	91249.143639	34.036480
908.107556	91400.879698	34.041498
909.106798	91573.958763	34.046516
909.993086	91748.823411	34.051533
911.085456	91890.923511	34.056551
912.045613	92075.619398	34.061568
913.122042	92231.710576	34.066586
913.922946	92387.544477	34.071604
915.495195	92535.980218	34.076621
916.546660	92692.964546	34.081639
917.365064	92860.082977	34.086656
918.309721	93015.637721	34.091674
919.207286	93164.682388	34.096692
919.869035	93329.310994	34.101709
921.171730	93484.626100	34.106727
921.853767	93641.386449	34.111744
922.760362	93806.775341	34.116762
923.773963	93967.153958	34.121780
924.555043	94142.046990	34.126797
925.529137	94296.700016	34.131815
926.124800	94463.821974	34.136832
926.893590	94625.998576	34.141850
927.829586	94797.016150	34.146868
929.094812	94967.904610	34.151885
929.969610	95143.846371	34.156903
931.068670	95303.865221	34.161920
931.812806	95465.500793	34.166938
932.530107	95637.484467	34.171956
933.253188	95805.208524	34.176973
934.703141	95978.118014	34.181991
935.547522	96148.546163	34.187008
936.767781	96304.013085	34.192026
937.613265	96481.773263	34.197044
938.533209	96648.343848	34.202061
939.501414	96816.395121	34.207079
940.745106	96979.958413	34.212096
941.885404	97130.474717	34.217114
942.729203	97305.861015	34.222132
943.607539	97460.929575	34.227149
944.384051	97619.972248	34.232167
945.296662	97796.597688	34.237184
946.640651	97942.381965	34.242202
947.707900	98103.304113	34.247220
948.440841	98272.410598	34.252237
949.292659	98429.129117	34.257255
950.019241	98601.625613	34.262272
951.306178	98752.741569	34.267290
952.310989	98903.158024	34.272308
953.275906	99055.474788	34.277325
954.435815	99200.809357	34.282343
954.886295	99351.383328	34.287360
956.051640	99497.725280	34.292378
956.848950	99641.001509	34.297396
957.571573	99808.727323	34.302413
958.796890	99951.029364	34.307431
959.638684	100111.799049	34.312448
960.626818	100261.498348	34.317466
961.770185	100419.871478	34.322484
962.482565	100571.789621	34.327501
963.388892	100730.596346	34.332519
964.064513	100896.026352	34.337536
964.851057	101060.495805	34.342554
965.868662	101228.410247	34.347572
966.593554	101393.170597	34.352589
967.902280	101557.696338	34.357607
968.548747	101739.578578	34.362624
970.008754	101911.653707	34.367642
971.147569	102083.371494	34.372660
971.985964	102254.614536	34.377677
973.278465	102419.889277	34.382695
974.418161	102590.711275	34.387712
975.186330	102753.345910	34.392730
976.490216	102910.397423	34.397748
976.932028	103076.627271	34.402765
978.035285	103245.420898	34.407783
978.483162	103435.521978	34.412800
979.763167	103616.046611	34.417818
980.777854	103791.588962	34.422836
981.251185	103966.405090	34.427853
982.586141	104151.717505	34.432871
983.535211	104329.313165	34.437888
984.207712	104521.202365	34.442906
984.848293	104707.627492	34.447924
985.803633	104904.949921	34.452941
986.901881	105091.466869	34.457959
987.907816	105293.425237	34.462976
988.685038	105483.854204	34.467994
989.461767	105692.609836	34.473012
990.771609	105885.841251	34.478029
992.238845	106077.946299	34.483047
992.810295	106274.417941	34.488064
993.810200	106465.197212	34.493082
995.125953	106667.665937	34.498100
995.925111	106859.342410	34.503117
997.014036	107050.313862	34.508135
997.859555	107262.591454	34.513152
998.675830	107454.434066	34.518170
999.933778	107663.835130	34.523188
1000.873645	107865.501192	34.528205
1002.245562	108051.253032	34.533223
1003.123850	108259.024308	34.538240
1003.870267	108463.120622	34.543258
1005.650439	108659.993039	34.548276
1006.426295	108842.695049	34.553293
1008.084804	109028.001082	34.558311
1008.974601	109211.890063	34.563328
1010.477014	109397.110431	34.568346
1011.949542	109562.717185	34.573364
1012.664626	109746.233359	34.578381
1013.953018	109919.801762	34.583399
1015.026022	110088.720288	34.588416
1015.633656	110255.474741	34.593434
1016.934825	110427.777665	34.598452
1017.611500	110606.695425	34.603469
1018.671215	110778.217117	34.608487
1019.409634	110955.480320	34.613504
1020.202332	111115.027462	34.618522
1021.344559	111287.628106	34.623540
1022.316456	111451.011052	34.628557
1023.163068	111613.718974	34.633575
1023.703689	111796.517834	34.638592
1024.755331	111973.355950	34.643610
1025.725259	112156.048343	34.648628
1026.609322	112345.824552	34.653645
1027.229838	112525.562252	34.658663
1028.253820	112724.767948	34.663680
1029.118744	112917.325479	34.668698
1030.111212	113103.871448	34.673716
1030.785471	113322.824939	34.678733
1032.307971	113523.613616	34.683751
1033.357622	113725.153225	34.688768
1034.128487	113922.154461	34.693786
1035.326724	114137.506166	34.698804
1036.023375	114335.574059	34.703821
1037.202581	114556.670919	34.708839
1038.398700	114761.145633	34.713856
1039.523376	114972.195991	34.718874
1040.704326	115171.190707	34.723892
1041.541290	115383.355848	34.728909
1042.760206	115582.879322	34.733927
1043.497685	115799.004068	34.738944
1044.654592	116017.062956	34.743962
1045.720570	116225.547971	34.748980
1046.972051	116434.295301	34.753997
1048.530699	116652.242120	34.759015
1049.367051	116863.481017	34.764032
1050.265338	117062.675178	34.769050
1051.941441	117269.660872	34.774068
1052.299418	117495.806972	34.779085
1053.591347	117702.833914	34.784103
1054.813952	117907.276472	34.789120
1055.384895	118123.877286	34.794138
1056.611185	118332.794817	34.799156
1057.570763	118558.229208	34.804173
1059.032768	118770.671367	34.809191
1060.206441	118982.060378	34.814208
1061.087615	119191.636669	34.819226
1062.422732	119413.455384	34.824244
1063.098250	119640.465655	34.829261
1064.604315	119850.691164	34.834279
1065.560234	120054.382149	34.839296
1066.750397	120267.437771	34.844314
1068.266355	120462.650990	34.849332
1069.163376	120680.243605	34.854349
1070.728685	120880.672015	34.859367
1071.802099	121066.547617	34.864384
1072.831045	121278.471520	34.869402
1074.121508	121472.664357	34.874420
1075.056237	121683.111517	34.879437
1076.373534	121872.157912	34.884455
1077.217335	122087.058079	34.889472
1078.453932	122278.553402	34.894490
1079.624996	122479.285970	34.899508
1080.529765	122675.856755	34.904525
1081.345340	122878.893684	34.909543
1082.118367	123091.734652	34.914560
1082.726611	123295.353578	34.919578
1084.271413	123504.192389	34.924596
1085.312262	123722.784968	34.929613
1086.073242	123932.960080	34.934631
1087.083478	124158.378763	34.939648
1087.972940	124359.031180	34.944666
1089.405207	124570.189834	34.949684
1089.740139	124785.992002	34.954701
1090.900103	124996.058054	34.959719
1092.342619	125197.511916	34.964736
1093.908434	125393.535327	34.969754
1095.320505	125593.311341	34.974772
1095.827574	125796.571172	34.979789
1096.821464	125999.333787	34.984807
1097.663894	126211.285729	34.989824
1098.935202	126414.043354	34.994842
1099.790189	126623.930316	34.999860
1100.838864	126852.277827	35.004877
1102.166913	127063.927443	35.009895
1103.132164	127270.568832	35.014912
1104.171457	127490.849366	35.019930
1105.437440	127716.696048	35.024948
1106.577425	127938.598157	35.029965
1107.426901	128143.578890	35.034983
1108.456604	128381.408708	35.040000
1109.299442	128613.808491	35.045018
1110.263502	128835.175769	35.050036
1111.167780	129077.518486	35.055053
1112.092509	129312.330887	35.060071
1113.016657	129559.756706	35.065088
1114.517650	129815.226640	35.070106
1115.921323	130060.473240	35.075124
1116.573160	130308.849912	35.080141
1117.736966	130544.582803	35.085159
1119.285133	130793.613916	35.090176
1120.170428	131050.437801	35.095194
1121.622932	131289.715823	35.100212
1122.338590	131541.412750	35.105229
1123.634148	131783.242904	35.110247
1125.028976	132040.662583	35.115264
1126.288260	132290.995484	35.120282
1127.590246	132521.054203	35.125300
1128.280463	132779.065214	35.130317
1129.665931	133020.382929	35.135335
1131.039921	133267.066489	35.140352
1132.487912	133505.639453	35.145370
1133.835196	133746.411199	35.150388
1134.759851	133990.081422	35.155405
1136.140369	134221.647970	35.160423
1138.084024	134452.134432	35.165440
1139.040084	134687.615495	35.170458
1140.274596	134925.156704	35.175476
1141.206564	135143.759223	35.180493
1142.054982	135381.025229	35.185511
1143.395977	135605.521647	35.190528
1144.238988	135851.082954	35.195546
1145.590287	136082.084480	35.200564
1146.627125	136311.225232	35.205581
1147.540506	136566.085664	35.210599
1148.772010	136805.086350	35.215616
1149.659464	137056.367055	35.220634
1150.685169	137299.208673	35.225652
1151.984216	137548.675631	35.230669
1152.710723	137791.418123	35.235687
1153.646584	138048.023221	35.240704
1154.449279	138303.206951	35.245722
1155.699973	138564.949527	35.250740
1156.283243	138830.303617	35.255757
1158.101983	139094.809266	35.260775
1159.275897	139357.115911	35.265792
1160.060896	139626.715762	35.270810
1161.377272	139891.183831	35.275828
1162.169698	140163.525415	35.280845
1163.640912	140422.735638	35.285863
1164.848948	140692.692594	35.290880
1165.601688	140956.361809	35.295898
1167.421686	141213.517166	35.300916
1168.295441	141457.631239	35.305933
1169.406652	141710.494859	35.310951
1170.548578	141963.824429	35.315968
1171.507924	142225.681502	35.320986
1173.223268	142469.460993	35.326004
1175.045447	142711.246496	35.331021
1176.469465	142960.796245	35.336039
1177.818473	143196.538759	35.341056
1179.030980	143436.451864	35.346074
1180.314144	143666.603759	35.351092
1181.193451	143911.748737	35.356109
1182.212940	144155.693009	35.361127
1183.678077	144418.801955	35.366144
1184.599923	144665.720494	35.371162
1185.588925	144917.740056	35.376180
1186.633116	145177.246737	35.381197
1187.517064	145426.028284	35.386215
1189.196526	145685.015367	35.391232
1190.048936	145955.820242	35.396250
1191.639118	146199.659119	35.401268
1192.749349	146463.691549	35.406285
1194.075591	146717.291477	35.411303
1195.358886	146967.374822	35.416320
1196.310842	147224.147107	35.421338
1197.523485	147493.902346	35.426356
1198.227270	147760.294142	35.431373
1199.285642	148037.104652	35.436391
1200.466391	148314.011220	35.441408
1201.593437	148601.442253	35.446426
1202.649836	148873.490998	35.451444
1203.834361	149158.621465	35.456461
1205.069526	149442.439511	35.461479
1206.404933	149739.496448	35.466496
1207.551665	150013.124079	35.471514
1208.341160	150297.770578	35.476532
1209.600407	150601.885958	35.481549
1210.731254	150890.906988	35.486567
1212.146565	151179.946731	35.491584
1213.220911	151482.577891	35.496602
1214.588642	151775.333582	35.501620
1216.022715	152061.396507	35.506637
1216.992254	152376.519905	35.511655
1218.128887	152664.259997	35.516672
1219.461376	152961.152898	35.521690
1220.329937	153260.217520	35.526708
1221.549293	153568.701415	35.531725
1223.078196	153880.371121	35.536743
1224.097912	154167.279411	35.541760
1225.916463	154483.434429	35.546778
1227.260716	154772.500725	35.551796
1228.953887	155060.446121	35.556813
1229.843076	155365.637648	35.561831
1231.454511	155656.416921	35.566848
1232.626871	155942.120898	35.571866
1234.078386	156239.323976	35.576884
1235.115390	156514.107593	35.581901
1236.408656	156811.696322	35.586919
1237.602689	157096.770926	35.591936
1239.090199	157393.355259	35.596954
1240.610813	157676.693043	35.601972
1241.825026	157956.036833	35.606989
1242.624725	158251.662885	35.612007
1244.548095	158520.301330	35.617024
1245.534108	158812.957775	35.622042
1246.420348	159097.437918	35.627060
1247.812002	159373.210377	35.632077
1248.918134	159654.880005	35.637095
1250.366426	159916.400692	35.642112
1251.431790	160196.583895	35.647130
1252.795049	160466.190443	35.652148
1253.966348	160737.949048	35.657165
1255.195903	161014.038537	35.662183
1256.580427	161274.868062	35.667200
1257.598195	161562.946706	35.672218
1258.536744	161838.899486	35.677236
1259.761657	162111.115059	35.682253
1260.899637	162410.623062	35.687271
1262.322757	162679.003661	35.692288
1263.490556	162974.032391	35.697306
1265.233258	163251.320830	35.702324
1266.756021	163538.340271	35.707341
1267.782749	163822.525520	35.712359
1269.143820	164089.098473	35.717376
1270.481098	164389.450482	35.722394
1271.828334	164666.978463	35.727412
1273.052806	164949.565425	35.732429
1274.222636	165242.820784	35.737447
1275.377964	165529.127751	35.742464
1276.319429	165833.044360	35.747482
1277.537028	166131.169984	35.752500
1278.704942	166429.077490	35.757517
1279.763973	166733.666187	35.762535
1281.433538	167050.692032	35.767552
1282.266466	167352.175751	35.772570
1283.444510	167673.981858	35.777588
1284.950371	167979.558633	35.782605
1285.984361	168298.652422	35.787623
1287.616391	168606.027160	35.792640
1288.194603	168939.170821	35.797658
1289.463719	169250.682959	35.802676
1290.982742	169582.356533	35.807693
1292.023208	169911.929067	35.812711
1293.544252	170229.814314	35.817728
1294.618086	170566.618835	35.822746
1295.911919	170893.225558	35.827764
1297.545727	171234.459951	35.832781
1298.860533	171560.040173	35.837799
1300.174080	171886.422352	35.842816
1301.595018	172222.268183	35.847834
1302.872417	172551.325841	35.852852
1304.335253	172874.822534	35.857869
1305.465273	173215.989811	35.862887
1307.003019	173549.110367	35.867904
1308.285253	173876.108149	35.872922
1309.554951	174217.614993	35.877940
1311.200812	174539.747848	35.882957
1312.560781	174873.478176	35.887975
1314.100189	175196.483306	35.892992
1315.878066	175524.210163	35.898010
1317.008451	175842.985128	35.903028
1318.379655	176157.128479	35.908045
1319.246842	176487.715298	35.913063
1320.839214	176805.519339	35.918080
1322.078023	177142.953044	35.923098
1323.041843	177462.400696	35.928116
1324.716240	177793.320022	35.933133
1325.763196	178122.314557	35.938151
1327.150824	178454.643596	35.943168
1328.154840	178796.988105	35.948186
1329.206262	179128.907563	35.953204
1330.998312	179461.024275	35.958221
1332.160474	179803.311497	35.963239
1333.552379	180134.648366	35.968256
1334.989921	180464.482255	35.973274
1336.260097	180785.791672	35.978292
1337.916276	181110.542349	35.983309
1338.939057	181431.820503	35.988327
1340.189180	181743.645693	35.993344
1341.414775	182075.403342	35.998362
1342.221768	182387.432462	36.003380
1344.052045	182708.242579	36.008397
1345.511545	183033.723158	36.013415
1346.996180	183361.270463	36.018432
1348.152220	183687.135166	36.023450
1349.487743	184017.579639	36.028468
1351.087238	184340.037029	36.033485
1352.216946	184675.736208	36.038503
1353.597430	185004.948176	36.043520
1354.938225	185337.176908	36.048538
1356.314498	185677.956850	36.053556
1357.394518	186005.333242	36.058573
1358.482138	186356.230607	36.063591
1359.961093	186699.716293	36.068608
1361.147620	187050.614456	36.073626
1362.382278	187410.874565	36.078644
1363.821292	187759.450739	36.083661
1365.136852	188111.172053	36.088679
1366.536378	188461.193467	36.093696
1368.530721	188823.672891	36.098714
1369.335247	189181.768558	36.103732
1370.953788	189542.956355	36.108749
1372.473954	189907.209192	36.113767
1373.243573	190267.564211	36.118784
1374.762901	190630.996640	36.123802
1375.996275	191011.856774	36.128820
1377.626147	191375.783358	36.133837
1379.241685	191742.354966	36.138855
1380.594454	192104.287994	36.143872
1382.219183	192480.231077	36.148890
1383.335967	192856.996631	36.153908
1384.943750	193216.558510	36.158925
1386.087373	193594.200164	36.163943
1387.547714	193958.906727	36.168960
1389.132154	194338.270196	36.173978
1390.268114	194711.248314	36.178996
1391.696731	195076.474534	36.184013
1393.328336	195458.452253	36.189031
1394.563696	195820.845642	36.194048
1396.309114	196194.569925	36.199066
1397.647927	196569.023671	36.204084
1399.260807	196948.791827	36.209101
1400.587604	197315.736289	36.214119
1401.790988	197688.492353	36.219136
1403.377630	198052.605109	36.224154
1404.906442	198419.459005	36.229172
1406.373078	198782.300675	36.234189
1407.828027	199156.699428	36.239207
1409.274211	199545.448052	36.244224
1410.769215	199904.558596	36.249242
1411.856134	200291.555322	36.254260
1413.122110	200651.913765	36.259277
1414.431227	201032.403058	36.264295
1416.310040	201412.483047	36.269312
1417.942609	201784.238928	36.274330
1419.346379	202154.092021	36.279348
1420.729539	202514.123460	36.284365
1421.734677	202901.986308	36.289383
1423.302935	203274.738348	36.294400
1424.592467	203645.875083	36.299418
1425.672484	204036.410743	36.304436
1427.714991	204405.103650	36.309453
1428.913334	204779.867146	36.314471
1430.464410	205153.736362	36.319488
1432.208022	205502.067571	36.324506
1433.820602	205849.406284	36.329524
1435.194710	206198.195344	36.334541
1436.510531	206539.491655	36.339559
1438.004071	206895.565077	36.344576
1439.245407	207249.764507	36.349594
1440.393647	207610.342280	36.354612
1441.799333	207972.199781	36.359629
1443.360941	208341.118393	36.364647
1444.652396	208715.390870	36.369664
1446.303724	209062.318768	36.374682
1447.519968	209445.723942	36.379700
1448.946083	209812.830649	36.384717
1449.962788	210192.386852	36.389735
1451.186278	210579.008757	36.394752
1452.828257	210951.951376	36.399770
1453.642936	211350.961273	36.404788
1454.830340	211737.493001	36.409805
1456.124030	212141.608404	36.414823
1457.352348	212546.295249	36.419840
1459.085432	212959.662430	36.424858
1460.436703	213381.475415	36.429876
1462.132929	213783.856016	36.434893
1463.566436	214206.497526	36.439911
1465.339083	214626.596225	36.444928
1466.808236	215038.416830	36.449946
1468.240292	215462.689963	36.454964
1469.972534	215872.718585	36.459981
1471.510133	216288.571729	36.464999
1472.798009	216700.785353	36.470016
1473.866071	217159.539764	36.475034
1475.491234	217623.969730	36.480052
1477.140633	218038.415348	36.485069
1478.795021	218463.198831	36.490087
1480.537004	218892.820721	36.495104
1481.848454	219307.200550	36.500122
1483.317057	219747.462254	36.505140
1484.809455	220171.797288	36.510157
1486.339072	220593.892914	36.515175
1487.719327	221029.755485	36.520192
1489.711806	221457.162755	36.525210
1490.585693	221882.216498	36.530228
1492.347286	222305.703142	36.535245
1494.139940	222743.536691	36.540263
1495.646319	223179.133355	36.545280
1497.408084	223600.466151	36.550298
1498.559479	224033.000703	36.555316
1500.285570	224469.505978	36.560333
1501.785630	224895.103125	36.565351
1503.261165	225331.805457	36.570368
1504.552502	225760.894574	36.575386
1505.683772	226197.377567	36.580404
1507.725903	226630.435302	36.585421
1509.393548	227050.907292	36.590439
1510.268860	227503.718543	36.595456
1512.424337	227925.662436	36.600474
1513.975199	228365.284371	36.605492
1515.296396	228798.875093	36.610509
1516.526476	229242.363011	36.615527
1517.979913	229680.430715	36.620544
1519.596848	230111.335380	36.625562
1521.043857	230561.218242	36.630580
1522.601486	231002.016335	36.635597
1524.083821	231435.157263	36.640615
1525.810089	231891.805767	36.645632
1527.803989	232322.350338	36.650650
1528.724865	232767.754968	36.655668
1529.730684	233194.426422	36.660685
1531.550023	233620.761654	36.665703
1532.767587	234052.531619	36.670720
1534.124113	234479.758458	36.675738
1535.493947	234928.753144	36.680756
1537.280820	235354.260265	36.685773
1538.529624	235799.670376	36.690791
1539.956844	236243.858386	36.695808
1541.413564	236685.426349	36.700826
1542.534103	237150.420392	36.705844
1544.296325	237601.008664	36.710861
1545.747620	238048.728188	36.715879
1547.090400	238522.655968	36.720896
1548.793866	238982.656039	36.725914
1549.957375	239459.918020	36.730932
1551.405914	239923.493291	36.735949
1553.124995	240402.698068	36.740967
1554.389092	240908.321030	36.745984
1556.088992	241375.617671	36.751002
1557.686012	241876.564846	36.756020
1558.958914	242361.893454	36.761037
1560.832673	242860.028354	36.766055
1562.169551	243351.140255	36.771072
1563.848055	243847.607527	36.776090
1565.789416	244339.231372	36.781108
1567.472193	244829.552514	36.786125
1569.190191	245321.951788	36.791143
1570.781352	245820.494933	36.796160
1572.526284	246306.236064	36.801178
1574.366125	246802.301268	36.806196
1576.144957	247281.154306	36.811213
1578.413125	247772.654154	36.816231
1579.775236	248246.319058	36.821248
1581.391382	248730.992975	36.826266
1583.001920	249220.418845	36.831284
1584.303268	249713.097172	36.836301
1586.369145	250191.475146	36.841319
1587.534839	250694.897174	36.846336
1589.236799	251168.103344	36.851354
1590.746428	251666.897243	36.856372
1592.366344	252156.045722	36.861389
1594.369613	252638.933089	36.866407
1595.778198	253137.389543	36.871424
1597.345655	253628.834372	36.876442
1598.966880	254120.677196	36.881460
1600.730952	254604.139186	36.886477
1602.667360	255107.108159	36.891495
1603.802194	255601.445616	36.896512
1605.288437	256091.635473	36.901530
1606.604106	256589.474719	36.906548
1608.355823	257086.708797	36.911565
1610.078272	257575.945887	36.916583
1611.488774	258084.947578	36.921600
1613.191415	258596.365351	36.926618
1614.769449	259093.298530	36.931636
1616.479222	259600.904859	36.936653
1618.215526	260098.091520	36.941671
1620.073339	260594.496068	36.946688
1621.766662	261091.867682	36.951706
1623.613752	261595.310692	36.956724
1625.028195	262091.635893	36.961741
1627.083194	262581.631513	36.966759
1628.556298	263082.062166	36.971776
1630.239293	263564.396307	36.976794
1631.671975	264063.893387	36.981812
1633.013852	264558.121363	36.986829
1634.495808	265053.443737	36.991847
1636.141571	265564.996890	36.996864
1638.012761	266033.301661	37.001882
1639.614178	266518.010315	37.006900
1641.011647	266994.445441	37.011917
1642.560345	267483.455233	37.016935
1643.909083	267958.119437	37.021952
1645.307151	268449.693578	37.026970
1647.319848	268956.382305	37.031988
1648.656841	269442.173656	37.037005
1650.295996	269935.230722	37.042023
1651.713278	270444.353142	37.047040
1653.304267	270936.985152	37.052058
1654.731803	271456.265806	37.057076
1656.404613	271977.435902	37.062093
1657.887087	272490.482325	37.067111
1659.219033	273017.575186	37.072128
1660.602457	273537.241097	37.077146
1662.610594	274065.440024	37.082164
1664.310389	274613.045766	37.087181
1666.446965	275135.607612	37.092199
1667.610984	275685.382724	37.097216
1669.253144	276220.090331	37.102234
1670.588090	276757.514797	37.107252
1671.964150	277314.542030	37.112269
1674.439313	277864.731239	37.117287
1675.576666	278415.343107	37.122304
1677.520384	278970.520041	37.127322
1679.375145	279523.525680	37.132340
1680.981945	280093.285420	37.137357
1682.351510	280647.257270	37.142375
1684.067325	281221.949324	37.147392
1685.845819	281776.739672	37.152410
1687.667927	282348.134040	37.157428
1689.431940	282918.977421	37.162445
1691.496947	283482.758502	37.167463
1693.374628	284050.709174	37.172480
1695.251400	284608.573744	37.177498
1697.303109	285177.711268	37.182516
1698.724241	285734.631225	37.187533
1700.574716	286303.925065	37.192551
1702.513527	286853.668794	37.197568
1704.291603	287427.898345	37.202586
1706.031005	287978.407595	37.207604
1707.553204	288541.701900	37.212621
1709.506696	289101.341374	37.217639
1710.968328	289671.067685	37.222656
1712.753107	290233.550013	37.227674
1714.451115	290801.835675	37.232692
1715.944431	291378.865053	37.237709
1717.664497	291935.559706	37.242727
1719.139496	292510.656730	37.247744
1721.259720	293080.488520	37.252762
1723.006096	293653.655999	37.257780
1725.172795	294227.005478	37.262797
1727.115669	294779.840835	37.267815
1729.243347	295351.388032	37.272832
1731.171779	295893.908359	37.277850
1733.354412	296447.305921	37.282868
1735.557885	296989.013728	37.287885
1737.258081	297522.318657	37.292903
1739.154005	298062.471847	37.297920
1740.644990	298599.666708	37.302938
1742.161391	299132.765504	37.307956
1744.092793	299671.355448	37.312973
1746.042537	300210.091985	37.317991
1747.743223	300746.453959	37.323008
1749.289997	301270.266401	37.328026
1750.715728	301821.373584	37.333044
1751.973979	302360.441332	37.338061
1753.812373	302879.727139	37.343079
1755.439359	303402.499113	37.348096
1756.974396	303928.839042	37.353114
1758.376915	304468.328325	37.358132
1759.746696	305000.480098	37.363149
1761.852606	305537.358193	37.368167
1763.424530	306078.765668	37.373184
1765.028389	306613.180511	37.378202
1767.097052	307148.201169	37.383220
1768.505610	307701.333535	37.388237
1770.382162	308244.683798	37.393255
1771.803719	308814.263666	37.398272
1773.376267	309361.567965	37.403290
1775.055943	309932.621454	37.408308
1776.698631	310503.423154	37.413325
1778.722368	311078.449840	37.418343
1780.562634	311660.918115	37.423360
1782.039740	312232.115873	37.428378
1784.342693	312802.995511	37.433396
1786.080112	313383.512674	37.438413
1787.935603	313961.339588	37.443431
1790.168102	314547.505457	37.448448
1791.681239	315128.198761	37.453466
1793.471084	315699.801695	37.458484
1795.279640	316301.844170	37.463501
1796.896367	316883.471600	37.468519
1798.473170	317478.076921	37.473536
1800.073550	318081.713362	37.478554
1802.180922	318680.588761	37.483572
1803.804998	319284.084066	37.488589
1805.130053	319887.801216	37.493607
1807.386225	320494.685855	37.498624
1808.392983	321129.016758	37.503642
1810.498350	321743.964346	37.508660
1812.101153	322371.634130	37.513677
1814.045654	322993.274653	37.518695
1815.733843	323631.709606	37.523712
1817.201429	324286.018474	37.528730
1819.313790	324917.896087	37.533748
1820.929071	325567.089367	37.538765
1822.405057	326200.303255	37.543783
1823.827131	326856.827333	37.548800
1826.708556	327516.632818	37.553818
1828.120629	328176.571994	37.558836
1829.887797	328829.590398	37.563853
1832.140279	329489.071877	37.568871
1834.105375	330154.356569	37.573888
1835.577664	330813.748834	37.578906
1837.854179	331452.056091	37.583924
1839.618939	332123.012780	37.588941
1841.721547	332774.510082	37.593959
1843.635178	333427.605040	37.598976
1845.973056	334078.312233	37.603994
1848.340051	334724.335932	37.609012
1849.855762	335372.904142	37.614029
1852.029679	336015.161978	37.619047
1854.104594	336653.417638	37.624064
1855.970821	337298.224092	37.629082
1857.852089	337924.235543	37.634100
1859.640155	338568.988664	37.639117
1861.508469	339205.876914	37.644135
1863.456322	339844.571868	37.649152
1864.838667	340499.191485	37.654170
1867.056993	341129.296977	37.659188
1868.528846	341791.424010	37.664205
1870.160125	342424.681490	37.669223
1872.010787	343077.946678	37.674240
1873.774379	343718.095184	37.679258
1875.575564	344346.350589	37.684276
1877.150436	344984.000889	37.689293
1878.859945	345614.742360	37.694311
1880.944590	346248.408567	37.699328
1882.437266	346882.722356	37.704346
1884.290504	347524.176041	37.709364
1885.737302	348173.555647	37.714381
1887.502095	348823.888917	37.719399
1889.752341	349478.295089	37.724416
1891.387082	350151.370453	37.729434
1893.779269	350793.984181	37.734452
1895.578522	351468.865473	37.739469
1897.246762	352129.800723	37.744487
1899.077487	352794.683546	37.749504
1900.812733	353474.823420	37.754522
1902.791832	354140.473521	37.759540
1904.686704	354823.864998	37.764557
1906.929873	355500.387646	37.769575
1908.751380	356183.896552	37.774592
1910.289202	356865.309842	37.779610
1912.559942	357549.686925	37.784628
1914.655111	358242.505901	37.789645
1916.538185	358938.317039	37.794663
1918.780678	359612.388803	37.799680
1920.608336	360303.390628	37.804698
1922.951854	360993.280810	37.809716
1924.577783	361678.457035	37.814733
1926.268156	362372.896829	37.819751
1928.157181	363071.021312	37.824768
1929.952084	363783.051962	37.829786
1932.008473	364478.485553	37.834804
1933.897893	365191.566045	37.839821
1935.705385	365902.490650	37.844839
1937.939702	366600.444653	37.849856
1939.538572	367332.179407	37.854874
1941.525684	368046.281840	37.859892
1943.094424	368773.935057	37.864909
1945.010722	369501.694462	37.869927
1946.849102	370222.426192	37.874944
1948.628676	370960.047055	37.879962
1950.976421	371691.471879	37.884980
1953.181398	372427.674182	37.889997
1954.967821	373162.002983	37.895015
1957.355207	373889.978364	37.900032
1959.432955	374642.389192	37.905050
1961.437040	375366.466553	37.910068
1963.345113	376105.026600	37.915085
1965.541078	376845.527241	37.920103
1967.454601	377582.711193	37.925120
1969.171774	378319.100395	37.930138
1971.238452	379050.318979	37.935156
1973.467075	379789.914543	37.940173
1975.075225	380537.077224	37.945191
1977.465338	381270.299713	37.950208
1979.342614	382020.377516	37.955226
1981.440546	382752.626941	37.960244
1983.473292	383489.460534	37.965261
1985.126712	384233.084947	37.970279
1987.479836	384966.840757	37.975296
1989.203950	385718.026447	37.980314
1991.856447	386454.640563	37.985332
1993.752490	387181.550855	37.990349
1995.600327	387917.021955	37.995367
1997.904854	388652.426165	38.000384
1999.728978	389399.452987	38.005402
2001.594571	390139.737255	38.010420
2003.601633	390880.056798	38.015437
2005.775816	391603.600261	38.020455
2008.090590	392309.790057	38.025472
2010.008028	393006.929017	38.030490
2011.750892	393719.137798	38.035508
2014.098183	394410.065019	38.040525
2015.845906	395120.896820	38.045543
2018.040390	395828.216458	38.050560
2020.089971	396530.930412	38.055578
2021.882827	397244.264523	38.060596
2024.235786	397950.874208	38.065613
2026.171139	398656.141978	38.070631
2028.332453	399370.453889	38.075648
2030.143934	400087.416392	38.080666
2031.788546	400808.950376	38.085684
2034.142643	401527.359095	38.090701
2035.663763	402264.031392	38.095719
2037.471464	402989.234403	38.100736
2039.096158	403733.833977	38.105754
2041.071248	404478.533615	38.110772
2043.138067	405233.257785	38.115789
2044.843517	405998.282998	38.120807
2047.140362	406755.664690	38.125824
2049.253322	407532.083546	38.130842
2050.907018	408292.772353	38.135860
2052.991139	409069.684730	38.140877
2055.189350	409851.116361	38.145895
2057.759579	410625.497547	38.150912
2059.426522	411406.693354	38.155930
2061.589762	412182.388977	38.160948
2063.876137	412962.322795	38.165965
2065.520861	413751.382550	38.170983
2067.995324	414544.740001	38.176000
2070.092048	415340.567452	38.181018
2072.031865	416121.377104	38.186036
2073.998479	416924.978886	38.191053
2075.995678	417725.435602	38.196071
2078.852808	418515.088898	38.201088
2080.374207	419314.536373	38.206106
2082.541534	420118.537307	38.211124
2084.927252	420914.348027	38.216141
2086.722168	421743.682233	38.221159
2089.153141	422539.408948	38.226176
2091.430711	423341.617844	38.231194
2093.289898	424138.046305	38.236212
2095.759869	424947.767692	38.241229
2097.651900	425757.811011	38.246247
2100.075764	426560.347174	38.251264
2101.495851	427385.402537	38.256282
2103.581081	428187.890339	38.261300
2105.929173	429016.838363	38.266317
2107.949903	429831.180242	38.271335
2110.007724	430647.969036	38.276352
2112.418366	431465.734793	38.281370
2114.597451	432286.244202	38.286388
2117.212805	433099.718026	38.291405
2119.334697	433914.308076	38.296423
2121.752944	434725.429486	38.301440
2124.350403	435526.876012	38.306458
2126.071907	436329.502165	38.311476
2128.286716	437141.028081	38.316493
2130.453779	437943.322012	38.321511
2132.323435	438753.430606	38.326528
2134.219212	439567.655830	38.331546
2136.213976	440383.100581	38.336564
2138.447226	441183.295424	38.341581
2140.378072	442019.388218	38.346599
2142.805346	442827.234335	38.351616
2144.495103	443662.698009	38.356634
2146.115769	444485.188939	38.361652
2147.956144	445290.815650	38.366669
2149.783253	446106.078082	38.371687
2151.654733	446914.220084	38.376704
2153.546263	447735.279393	38.381722
2155.829809	448563.476778	38.386740
2158.085169	449383.755749	38.391757
2159.781920	450211.480526	38.396775
2161.872044	451040.018791	38.401792
2164.064448	451893.847828	38.406810
2165.820168	452742.150975	38.411828
2168.181471	453599.625817	38.416845
2169.833767	454466.234977	38.421863
2171.792698	455332.201309	38.426880
2173.882328	456203.773635	38.431898
2176.344104	457074.843324	38.436916
2178.546109	457969.431229	38.441933
2180.695654	458856.808952	38.446951
2183.308877	459718.791810	38.451968
2185.870519	460610.979910	38.456986
2188.119388	461504.444072	38.462004
2190.207554	462390.312117	38.467021
2192.364740	463287.452945	38.472039
2194.582396	464165.891075	38.477056
2196.773487	465077.200239	38.482074
2199.085852	465983.291909	38.487092
2201.077993	466878.123897	38.492109
2203.281686	467793.651691	38.497127
2205.560246	468710.235948	38.502144
2207.546604	469618.284789	38.507162
2209.448347	470544.041616	38.512180
2211.861776	471464.464970	38.517197
2214.058639	472392.105150	38.522215
2215.956426	473326.368216	38.527232
2218.479392	474268.414157	38.532250
2220.340697	475213.098707	38.537268
2222.798747	476153.596041	38.542285
2225.313069	477111.868426	38.547303
2227.393629	478059.606080	38.552320
2229.728378	479020.688852	38.557338
2231.629223	479965.681548	38.562356
2234.167541	480903.652012	38.567373
2236.364803	481873.951531	38.572391
2238.669810	482835.394846	38.577408
2240.873478	483803.317895	38.582426
2242.814235	484783.249810	38.587444
2245.498325	485745.485546	38.592461
2247.382789	486711.739443	38.597479
2250.182868	487679.506469	38.602496
2252.528236	488657.139717	38.607514
2254.763977	489629.285147	38.612532
2257.044847	490590.718815	38.617549
2259.436832	491565.557907	38.622567
2262.267387	492534.163173	38.627584
2264.921883	493477.408326	38.632602
2267.299793	494437.402172	38.637620
2269.410626	495393.248572	38.642637
2271.585629	496348.526492	38.647655
2273.851578	497301.667216	38.652672
2276.280522	498259.369410	38.657690
2278.626973	499221.420287	38.662708
2281.357448	500166.755381	38.667725
2283.362419	501127.391448	38.672743
2285.489358	502072.062746	38.677760
2287.954274	503021.416516	38.682778
2290.212221	503969.842196	38.687796
2292.785175	504920.229275	38.692813
2295.231124	505864.883659	38.697831
2297.662044	506789.012156	38.702848
2300.303871	507708.918659	38.707866
2302.484049	508618.865534	38.712884
2304.853453	509514.713366	38.717901
2307.041643	510419.767659	38.722919
2309.048895	511317.742840	38.727936
2311.560834	512219.718198	38.732954
2313.444756	513126.635738	38.737972
2315.513680	514032.009277	38.742989
2317.643395	514958.792600	38.748007
2319.617296	515894.467928	38.753024
2321.856989	516820.317173	38.758042
2323.334714	517771.081403	38.763060
2325.648206	518718.928809	38.768077
2327.835858	519685.281743	38.773095
2329.612580	520661.315888	38.778112
2332.025614	521633.354386	38.783130
2333.996693	522621.928176	38.788148
2336.107507	523606.687337	38.793165
2338.261326	524613.438409	38.798183
2340.488112	525617.995232	38.803200
2343.415808	526631.989381	38.808218
2345.130433	527647.777167	38.813236
2347.614310	528670.318712	38.818253
2350.177815	529709.091910	38.823271
2352.430467	530731.630917	38.828288
2354.741295	531769.546386	38.833306
2357.128888	532824.140654	38.838324
2359.709831	533866.596144	38.843341
2362.270655	534905.457190	38.848359
2364.600130	535953.140965	38.853376
2367.411675	537003.135844	38.858394
2369.743445	538047.497168	38.863412
2372.103581	539098.823211	38.868429
2374.762843	540145.192410	38.873447
2376.972521	541201.672376	38.878464
2379.672918	542258.747749	38.883482
2381.850178	543322.873585	38.888500
2384.369667	544369.709499	38.893517
2386.512450	545431.317712	38.898535
2389.001327	546504.607967	38.903552
2391.441482	547567.916319	38.908570
2393.762278	548647.456354	38.913588
2396.545305	549717.081021	38.918605
2398.616007	550792.220768	38.923623
2400.720050	551861.438949	38.928640
2403.417506	552945.658036	38.933658
2406.139905	554023.754685	38.938676
2409.589854	555077.418544	38.943693
2412.303815	556133.685007	38.948711
2414.865121	557192.808799	38.953728
2417.365315	558249.698351	38.958746
2419.507356	559319.527612	38.963764
2421.402315	560371.173602	38.968781
2423.563254	561449.420415	38.973799
2426.135822	562528.466056	38.978816
2428.960331	563579.302118	38.983834
2430.687353	564674.586487	38.988852
2433.118269	565750.628371	38.993869
2435.445453	566830.515729	38.998887
2437.576818	567927.418907	39.003904
2439.872651	569008.134450	39.008922
2441.983866	570113.993803	39.013940
2444.416112	571198.268532	39.018957
2446.693351	572308.178572	39.023975
2448.981339	573424.716253	39.028992
2451.657683	574529.799155	39.034010
2453.680014	575645.281732	39.039028
2456.528376	576738.901582	39.044045
2459.533193	577812.179333	39.049063
2462.199781	578888.983050	39.054080
2464.857570	579954.256995	39.059098
2467.384803	581012.638923	39.064116
2470.020561	582070.962691	39.069133
2472.524160	583134.533940	39.074151
2474.636819	584192.962312	39.079168
2477.628273	585256.369653	39.084186
2479.797324	586320.722540	39.089204
2482.100384	587394.686967	39.094221
2484.409124	588463.842877	39.099239
2486.508133	589545.721608	39.104256
2488.954336	590640.728831	39.109274
2490.900863	591731.608750	39.114292
2493.028832	592838.345933	39.119309
2495.255732	593959.245451	39.124327
2497.639729	595081.215828	39.129344
2500.404825	596224.961067	39.134362
2502.640862	597362.220239	39.139380
2504.806709	598500.883639	39.144397
2507.359943	599652.945725	39.149415
2509.242287	600813.217894	39.154432
2511.940266	601983.555428	39.159450
2514.368399	603167.388332	39.164468
2516.520460	604356.952883	39.169485
2519.291510	605547.794115	39.174503
2521.581046	606760.014466	39.179520
2524.286670	607946.762309	39.184538
2526.854782	609163.986127	39.189556
2529.146654	610387.980008	39.194573
2532.192622	611589.201664	39.199591
2534.197469	612817.081616	39.204608
2536.966934	614044.200697	39.209626
2539.120189	615273.487149	39.214644
2541.501093	616511.302179	39.219661
2544.481215	617751.180367	39.224679
2546.966853	619008.150847	39.229696
2549.116757	620248.334723	39.234714
2552.000555	621517.250777	39.239732
2554.499324	622774.036778	39.244749
2557.554134	624034.683939	39.249767
2559.593533	625295.901382	39.254784
2563.015346	626560.990597	39.259802
2565.413335	627829.147176	39.264820
2568.064307	629091.517045	39.269837
2570.869956	630359.256247	39.274855
2573.350628	631621.404189	39.279872
2576.067468	632883.163026	39.284890
2578.572253	634152.245480	39.289908
2581.433469	635414.176544	39.294925
2584.390260	636675.390699	39.299943
2586.717869	637948.085756	39.304960
2589.923826	639207.205332	39.309978
2592.409867	640463.645834	39.314996
2595.244668	641724.116877	39.320013
2598.079814	642992.116051	39.325031
2600.078134	644242.488171	39.330048
2602.661008	645494.456247	39.335066
2605.202362	646770.663080	39.340084
2607.905206	648040.998321	39.345101
2610.631841	649304.738431	39.350119
2613.150383	650580.916438	39.355136
2615.580104	651855.202206	39.360154
2618.013649	653125.238236	39.365172
2620.350064	654401.905369	39.370189
2623.145263	655676.240044	39.375207
2626.146150	656955.308617	39.380224
2628.474919	658217.385965	39.385242
2631.059613	659461.428619	39.390260
2633.616945	660698.843771	39.395277
2636.685067	661919.436732	39.400295
2638.973661	663173.461488	39.405312
2641.634844	664402.870289	39.410330
2644.199233	665649.907753	39.415348
2646.937291	666888.742471	39.420365
2649.734573	668125.864827	39.425383
2651.861955	669390.153126	39.430400
2654.395277	670639.680429	39.435418
2656.765411	671911.702417	39.440436
2658.914526	673190.652137	39.445453
2661.690296	674461.468182	39.450471
2663.681327	675762.372552	39.455488
2666.611381	677065.029477	39.460506
2669.390389	678352.319171	39.465524
2671.755501	679661.814237	39.470541
2674.860044	680971.847246	39.475559
2677.283536	682302.426322	39.480576
2679.690689	683626.854363	39.485594
2682.255641	684965.072532	39.490612
2684.626205	686318.175053	39.495629
2687.545952	687656.089114	39.500647
2689.701863	689020.295641	39.505664
2692.263441	690383.782833	39.510682
2695.273438	691754.832088	39.515700
2697.976719	693126.615890	39.520717
2700.924724	694512.141651	39.525735
2703.363647	695898.776356	39.530752
2706.313442	697282.779175	39.535770
2708.594319	698679.917967	39.540788
2711.079747	700074.421666	39.545805
2714.198693	701486.944336	39.550823
2716.834559	702902.342769	39.555840
2719.624288	704322.641011	39.560858
2722.462592	705741.510035	39.565876
2724.982942	707168.473630	39.570893
2727.602091	708597.265858	39.575911
2730.120733	710029.601816	39.580928
2732.915305	711468.239591	39.585946
2735.660260	712921.943221	39.590964
2738.766379	714357.368561	39.595981
2741.521118	715799.390075	39.600999
2744.387265	717262.476942	39.606016
2747.090706	718701.437550	39.611034
2750.194375	720164.425605	39.616052
2753.058761	721609.093696	39.621069
2756.106578	723047.052036	39.626087
2758.753768	724500.897333	39.631104
2761.563763	725951.197537	39.636122
2764.525977	727399.883014	39.641140
2767.543481	728847.710932	39.646157
2770.457079	730280.674290	39.651175
2773.112855	731734.869122	39.656192
2775.847218	733188.939134	39.661210
2778.988167	734626.680604	39.666228
2781.455638	736083.336129	39.671245
2784.459492	737523.151074	39.676263
2787.175861	738968.381696	39.681280
2789.732941	740427.737788	39.686298
2792.622167	741871.723062	39.691316
2795.636814	743336.883920	39.696333
2798.126666	744773.697089	39.701351
2801.210015	746229.826399	39.706368
2804.187999	747681.709557	39.711386
2807.197162	749125.283306	39.716404
2809.999592	750569.757593	39.721421
2813.123569	751995.185570	39.726439
2815.831630	753406.822117	39.731456
2818.722379	754803.885654	39.736474
2821.558026	756186.126903	39.741492
2824.048992	757595.849241	39.746509
2827.021662	758983.127471	39.751527
2830.181842	760364.314126	39.756544
2832.229294	761764.478834	39.761562
2835.175379	763158.578223	39.766580
2837.617145	764566.819225	39.771597
2840.343534	765986.849682	39.776615
2842.757834	767413.498396	39.781632
2845.317317	768851.405377	39.786650
2847.972336	770303.520788	39.791668
2850.563259	771752.463242	39.796685
2853.788986	773198.265858	39.801703
2856.975895	774657.695085	39.806720
2859.698508	776125.114148	39.811738
2863.037042	777577.945541	39.816756
2865.422320	779053.083562	39.821773
2868.362516	780526.309685	39.826791
2870.920862	782018.686085	39.831808
2873.641799	783497.135804	39.836826
2876.429454	785000.193422	39.841844
2879.509155	786492.882714	39.846861
2882.830515	787996.009618	39.851879
2885.539239	789493.086692	39.856896
2888.269895	791001.560471	39.861914
2891.810898	792517.078025	39.866932
2894.331888	794035.868490	39.871949
2897.079308	795560.711447	39.876967
2899.920897	797076.392214	39.881984
2902.453697	798612.850456	39.887002
2905.614293	800153.223729	39.892020
2907.952412	801698.040781	39.897037
2910.692034	803252.135797	39.902055
2913.576367	804823.860070	39.907072
2916.450458	806395.129234	39.912090
2919.512936	807960.775233	39.917108
2921.971102	809547.819144	39.922125
2925.006933	811132.785229	39.927143
2928.220494	812715.299645	39.932160
2931.106881	814330.131333	39.937178
2933.822120	815923.700517	39.942196
2936.387678	817544.895576	39.947213
2940.084825	819133.633849	39.952231
2943.058281	820739.097467	39.957248
2946.019082	822344.029167	39.962266
2949.076935	823956.458893	39.967284
2952.005935	825588.365603	39.972301
2954.653779	827196.753940	39.977319
2957.762145	828830.556156	39.982336
2960.549741	830442.657422	39.987354
2963.859896	832062.946114	39.992372
2966.626075	833701.234785	39.997389
2969.339240	835320.466329	40.002407
2972.518230	836954.550239	40.007424
2975.374353	838595.426613	40.012442
2978.755459	840227.572490	40.017460
2981.057571	841855.830122	40.022477
2984.528094	843514.702084	40.027495
2987.418320	845142.117217	40.032512
2990.430628	846795.731071	40.037530
2993.237956	848435.823163	40.042548
2995.811225	850096.027570	40.047565
2998.852122	851737.257058	40.052583
3002.174214	853397.139912	40.057600
3005.021012	855046.851196	40.062618
3008.113296	856695.499890	40.067636
3010.644146	858329.147502	40.072653
3013.353235	859939.048387	40.077671
3016.310781	861567.785937	40.082688
3018.970434	863199.143962	40.087706
3021.807887	864828.581400	40.092724
3024.414154	866468.182397	40.097741
3027.177186	868118.551394	40.102759
3030.517405	869776.024943	40.107776
3033.046990	871443.341664	40.112794
3035.872066	873115.856606	40.117812
3038.455845	874812.523218	40.122829
3041.238847	876489.807051	40.127847
3044.401564	878195.666150	40.132864
3047.303912	879913.258397	40.137882
3050.390743	881626.355671	40.142900
3053.514305	883361.365657	40.147917
3056.317174	885091.469436	40.152935
3059.539707	886827.750458	40.157952
3062.592089	888586.421851	40.162970
3065.402223	890323.460736	40.167988
3068.241533	892092.874088	40.173005
3071.863279	893852.160331	40.178023
3075.293880	895627.908743	40.183040
3078.376297	897405.860684	40.188058
3081.506336	899180.453763	40.193076
3084.737537	900948.019302	40.198093
3087.898895	902743.453665	40.203111
3091.085035	904519.055091	40.208128
3094.147197	906313.748667	40.213146
3097.402468	908109.854095	40.218164
3100.513593	909903.864476	40.223181
3103.671090	911700.652087	40.228199
3106.698858	913488.129570	40.233216
3109.833493	915292.497692	40.238234
3112.995555	917096.459968	40.243252
3116.117646	918914.909864	40.248269
3118.946389	920726.849378	40.253287
3122.516802	922548.521920	40.258304
3125.656688	924370.707108	40.263322
3128.802475	926178.561878	40.268340
3131.502789	928006.588608	40.273357
3134.947504	929832.814269	40.278375
3138.389133	931668.761519	40.283392
3141.369485	933496.393411	40.288410
3144.811989	935318.627537	40.293428
3147.878810	937157.137672	40.298445
3151.076037	938991.252600	40.303463
3154.629861	940821.415329	40.308480
3157.329810	942651.364097	40.313498
3160.830359	944474.325720	40.318516
3164.261656	946303.727331	40.323533
3167.433127	948145.702944	40.328551
3170.756913	949958.259751	40.333568
3173.895251	951812.959920	40.338586
3176.931124	953651.454798	40.343604
3180.594814	955505.933946	40.348621
3183.511723	957389.834366	40.353639
3186.742555	959265.832173	40.358656
3189.671842	961151.435980	40.363674
3192.711785	963037.870500	40.368692
3195.886508	964921.808720	40.373709
3198.566538	966818.786029	40.378727
3201.798226	968719.927799	40.383744
3204.707316	970628.984028	40.388762
3207.939062	972530.327641	40.393780
3211.187644	974450.933736	40.398797
3213.605934	976357.870741	40.403815
3217.128262	978268.181507	40.408832
3220.019098	980169.091884	40.413850
3223.054302	982034.769499	40.418868
3225.987040	983929.453770	40.423885
3228.808838	985821.677563	40.428903
3232.034950	987716.417412	40.433920
3235.025143	989622.821506	40.438938
3238.175165	991525.643274	40.443956
3241.385676	993440.551747	40.448973
3244.543463	995369.690322	40.453991
3248.184688	997284.493949	40.459008
3251.652462	999206.544782	40.464026
3255.213922	1001130.160481	40.469044
3258.628937	1003069.934050	40.474061
3261.593838	1005009.310145	40.479079
3264.904121	1006937.684357	40.484096
3267.605631	1008901.076488	40.489114
3270.424453	1010860.180104	40.494132
3273.523875	1012837.058545	40.499149
3276.298700	1014820.074599	40.504167
3279.833830	1016817.754463	40.509184
3282.838948	1018830.100468	40.514202
3285.789542	1020852.858169	40.519220
3289.096946	1022871.829709	40.524237
3292.531997	1024910.351711	40.529255
3296.167411	1026947.228430	40.534272
3298.930607	1029001.955786	40.539290
3302.390357	1031049.826047	40.544308
3305.495033	1033103.663141	40.549325
3308.522072	1035172.290492	40.554343
3311.989888	1037247.214135	40.559360
3315.242843	1039334.318696	40.564378
3318.678505	1041412.995674	40.569396
3322.035592	1043507.574390	40.574413
3325.108044	1045616.047337	40.579431
3328.711690	1047719.394841	40.584448
3331.971223	1049838.744041	40.589466
3335.130219	1051952.487997	40.594484
3338.729019	1054066.312460	40.599501
3342.242254	1056171.747967	40.604519
3345.737553	1058297.040442	40.609536
3349.074510	1060437.482662	40.614554
3352.333124	1062552.046961	40.619572
3355.556341	1064688.453111	40.624589
3359.035261	1066823.602344	40.629607
3362.208915	1068948.381188	40.634624
3365.391984	1071106.652546	40.639642
3368.933168	1073250.024202	40.644660
3372.456421	1075399.551113	40.649677
3375.693950	1077544.928316	40.654695
3378.934841	1079701.999610	40.659712
3382.421793	1081865.639393	40.664730
3385.678193	1084010.956912	40.669748
3388.912265	1086178.853129	40.674765
3392.409507	1088352.530407	40.679783
3396.177986	1090513.926193	40.684800
3399.158288	1092694.736902	40.689818
3402.816000	1094870.072678	40.694836
3406.180862	1097039.907714	40.699853
3409.209301	1099224.567382	40.704871
3412.776342	1101399.866133	40.709888
3415.973044	1103596.360481	40.714906
3419.517614	1105770.185759	40.719924
3423.240668	1107951.006560	40.724941
3426.226719	1110138.392809	40.729959
3429.507818	1112328.360033	40.734976
3432.928778	1114518.932287	40.739994
3436.431914	1116723.804952	40.745012
3439.683073	1118881.177126	40.750016
3442.984841	1121022.504916	40.755021
3446.890959	1123082.634937	40.760026
3449.587150	1125089.361739	40.765031
3452.598341	1127015.671246	40.770036
3455.864370	1128881.436534	40.775040
3458.552095	1130675.356561	40.780045
3461.202048	1132366.343060	40.785050
3464.218158	1134008.666590	40.790055
3466.823583	1135551.125201	40.795060
3469.555573	1137031.121873	40.800064
3472.096527	1138453.601173	40.805069
3474.765808	1139772.346796	40.810074
3476.877550	1141036.024621	40.815079
3478.828596	1142220.044267	40.820084
3481.209035	1143334.507875	40.825088
3482.533391	1144405.964521	40.830093
3485.004260	1145385.168147	40.835098
3486.393002	1146310.729105	40.840103
3487.966109	1147186.636174	40.845108
3489.485817	1148012.953127	40.850112
3491.039450	1148788.552113	40.855117
3492.314163	1149501.289111	40.860122
3493.807863	1150181.601056	40.865127
3495.197572	1150793.761344	40.870132
3496.900310	1151377.584806	40.875136
3498.027951	1151921.961530	40.880141
3499.233265	1152394.801223	40.885146
3500.186405	1152845.680717	40.890151
3501.139246	1153253.837028	40.895156
3502.511100	1153624.889317	40.900160
3503.333914	1153969.319723	40.905165
3504.181027	1154271.709616	40.910170
3505.191322	1154548.034413	40.915175
3505.940205	1154791.839575	40.920180
3506.856066	1154989.434760	40.925184
3507.451471	1155179.506487	40.930189
3508.558564	1155327.197741	40.935194
3509.098541	1155454.354368	40.940199
3509.417861	1155570.002701	40.945204
3510.550106	1155652.120378	40.950208
3510.999440	1155717.037401	40.955213
3511.493296	1155770.121377	40.960218
3512.289973	1155772.071543	40.965223
3512.601490	1155769.655439	40.970228
3513.008165	1155750.668736	40.975232
3513.373346	1155711.444343	40.980237
3514.225351	1155653.786830	40.985242
3514.569714	1155598.009738	40.990247
3514.688409	1155507.549628	40.995252
3515.071061	1155412.408808	41.000256
3515.114531	1155307.009898	41.005261
3515.466744	1155186.988128	41.010266
3516.147887	1155047.608560	41.015271
3515.933345	1154909.413575	41.020276
3516.522463	1154741.940377	41.025280
3516.882994	1154585.759370	41.030285
3517.135186	1154408.206617	41.035290
3517.710647	1154221.510426	41.040295
3517.351783	1154025.498419	41.045300
3517.713349	1153826.521427	41.050304
3517.891027	1153624.444146	41.055309
3518.474194	1153398.915795	41.060314
3518.702532	1153167.852098	41.065319
3518.360644	1152928.448282	41.070324
3518.974476	1152701.938520	41.075328
3519.013474	1152457.055220	41.080333
3519.048769	1152198.150940	41.085338
3518.835079	1151951.013787	41.090343
3519.027916	1151689.975874	41.095348
3519.274679	1151419.543068	41.100352
3519.587048	1151156.376121	41.105357
3519.682446	1150880.354304	41.110362
3520.139335	1150600.754878	41.115367
3519.789896	1150307.352884	41.120372
3520.312926	1150020.135951	41.125376
3519.929437	1149735.136241	41.130381
3520.239148	1149431.822022	41.135386
3520.109395	1149131.783171	41.140391
3520.181654	1148827.999731	41.145396
3520.556584	1148525.664620	41.150400
3520.226312	1148212.060105	41.155405
3520.493057	1147906.770549	41.160410
3520.411274	1147586.077075	41.165415
3520.600793	1147276.405429	41.170420
3520.695926	1146951.380404	41.175424
3520.656959	1146635.833814	41.180429
3521.031585	1146304.184226	41.185434
3521.044889	1145984.041137	41.190439
3520.618283	1145655.420790	41.195444
3520.910272	1145322.680585	41.200448
3520.803170	1144995.198770	41.205453
3521.111856	1144651.227948	41.210458
3521.162486	1144325.574637	41.215463
3520.922110	1143977.858214	41.220468
3520.894551	1143629.325322	41.225472
3520.784273	1143295.860029	41.230477
3521.293335	1142951.271477	41.235482
3521.137422	1142608.097698	41.240487
3520.855371	1142267.577998	41.245492
3520.881868	1141920.251346	41.250496
3520.900390	1141572.903208	41.255501
3521.194229	1141235.067841	41.260506
3521.095845	1140875.076711	41.265511
3520.788946	1140537.200876	41.270516
3521.292500	1140180.668568	41.275520
3520.873964	1139837.548106	41.280525
3520.754016	1139480.786715	41.285530
3521.155350	1139144.982813	41.290535
3520.944113	1138775.377729	41.295540
3521.219334	1138422.560896	41.300544
3520.880015	1138072.954055	41.305549
3521.016175	1137717.835211	41.310554
3520.873030	1137367.105352	41.315559
3520.744994	1137009.514410	41.320564
3520.952985	1136649.280568	41.325568
3521.147007	1136302.032564	41.330573
3521.085851	1135946.827639	41.335578
3521.255661	1135574.752693	41.340583
3521.278425	1135225.563224	41.345588
3521.095882	1134861.568594	41.350592
3520.934263	1134513.312387	41.355597
3520.767609	1134140.622457	41.360602
3520.603627	1133782.535000	41.365607
3520.605495	1133427.056093	41.370612
3520.897204	1133068.560466	41.375616
3520.839811	1132709.623089	41.380621
3520.666670	1132354.291270	41.385626
3520.679506	1131991.683108	41.390631
3520.532595	1131630.311946	41.395636
3520.912103	1131279.473857	41.400640
3520.488925	1130931.311038	41.405645
3520.748150	1130568.375164	41.410650
3520.814021	1130204.590861	41.415655
3520.650339	1129843.766488	41.420660
3520.472173	1129477.405934	41.425664
3520.234719	1129131.186276	41.430669
3520.237055	1128763.225613	41.435674
3520.161307	1128424.254779	41.440679
3520.109754	1128058.441356	41.445684
3520.552424	1127712.017419	41.450688
3520.041028	1127351.937349	41.455693
3520.034792	1127001.546590	41.460698
3520.220014	1126639.496466	41.465703
3519.978238	1126291.000219	41.470708
3519.964352	1125925.700073	41.475712
3519.732567	1125580.390290	41.480717
3519.563909	1125238.568168	41.485722
3519.937024	1124877.128616	41.490727
3519.802808	1124531.544558	41.495732
3520.083625	1124171.880466	41.500736
3520.066026	1123834.130767	41.505741
3520.121969	1123482.451658	41.510746
3520.054349	1123116.777670	41.515751
3519.661852	1122759.128160	41.520756
3519.730868	1122422.321981	41.525760
3519.444081	1122071.367957	41.530765
3519.682240	1121712.211637	41.535770
3519.544771	1121366.328005	41.540775
3519.689861	1121009.139292	41.545780
3519.588268	1120660.918779	41.550784
3519.693532	1120313.689092	41.555789
3519.396508	1119954.693295	41.560794
3519.502641	1119609.417789	41.565799
3519.330904	1119257.879069	41.570804
3519.326521	1118908.290127	41.575808
3519.246107	1118571.170623	41.580813
3519.373356	1118217.132652	41.585818
3519.313932	1117866.532009	41.590823
3518.874968	1117533.503136	41.595828
3519.476716	1117176.364403	41.600832
3519.261290	1116831.153184	41.605837
3519.399981	1116478.427807	41.610842
3519.217217	1116138.694119	41.615847
3518.905406	1115792.955321	41.620852
3519.401873	1115438.291575	41.625856
3519.198053	1115096.112230	41.630861
3519.312674	1114737.651942	41.635866
3519.383539	1114383.655866	41.640871
3519.060078	1114047.721725	41.645876
3519.194227	1113690.427716	41.650880
3518.801304	1113351.124059	41.655885
3518.702508	1113007.840568	41.660890
3519.007453	1112667.234358	41.665895
3518.712705	1112323.462510	41.670900
3518.968224	1111973.664304	41.675904
3518.611493	1111634.818449	41.680909
3518.793803	1111301.395311	41.685914
3518.609419	1110958.567222	41.690919
3518.393324	1110618.966296	41.695924
3518.561998	1110274.796137	41.700928
3518.232390	1109936.411124	41.705933
3518.243110	1109603.865078	41.710938
3518.265927	1109276.545141	41.715943
3518.066399	1108935.403623	41.720948
3518.289436	1108595.888830	41.725952
3517.995817	1108274.954676	41.730957
3518.318181	1107933.472748	41.735962
3518.294604	1107599.567483	41.740967
3518.164167	1107264.322568	41.745972
3518.033040	1106937.649358	41.750976
3518.128717	1106598.411370	41.755981
3518.340520	1106266.103203	41.760986
3518.147013	1105929.257772	41.765991
3517.850637	1105601.384802	41.770996
3517.772698	1105263.810238	41.776000
3517.710808	1104937.577263	41.781005
3517.880936	1104609.853622	41.786010
3518.126750	1104290.789808	41.791015
3517.704472	1103944.306010	41.796020
3517.852329	1103612.704401	41.801024
3517.660866	1103291.742847	41.806029
3517.693009	1102966.330411	41.811034
3517.855642	1102637.532664	41.816039
3517.805171	1102309.705512	41.821044
3517.704076	1101972.215227	41.826048
3517.344536	1101650.419178	41.831053
3517.284476	1101325.018468	41.836058
3517.344327	1101002.445702	41.841063
3517.116847	1100681.430305	41.846068
3517.430721	1100350.843390	41.851072
3516.957625	1100040.153872	41.856077
3516.911719	1099723.735733	41.861082
3517.164004	1099403.043307	41.866087
3516.894200	1099090.544769	41.871092
3517.036193	1098770.119773	41.876096
3516.918480	1098462.723164	41.881101
3516.905502	1098135.018752	41.886106
3516.974004	1097828.129148	41.891111
3517.022094	1097508.983715	41.896116
3517.108475	1097188.091536	41.901120
3516.945787	1096888.646956	41.906125
3516.610775	1096557.839177	41.911130
3516.542369	1096247.056152	41.916135
3516.581487	1095933.654560	41.921140
3516.616112	1095624.445138	41.926144
3516.447546	1095319.844041	41.931149
3516.471173	1095001.128722	41.936154
3516.400540	1094700.591024	41.941159
3516.469452	1094393.410777	41.946164
3516.834585	1094075.445970	41.951168
3516.460466	1093765.623486	41.956173
3516.824868	1093460.542882	41.961178
3516.763450	1093152.260891	41.966183
3516.489106	1092831.935517	41.971188
3516.407614	1092518.738980	41.976192
3516.012724	1092215.532145	41.981197
3516.211620	1091904.742992	41.986202
3516.336338	1091605.916163	41.991207
3515.838706	1091304.302906	41.996212
3516.025924	1090992.888922	42.001216
3516.028373	1090699.394501	42.006221
3515.993221	1090392.866414	42.011226
3516.262088	1090095.464857	42.016231
3516.138507	1089785.852401	42.021236
3515.826384	1089477.306920	42.026240
3515.988961	1089181.309487	42.031245
3515.751699	1088876.453171	42.036250
3515.891553	1088590.676953	42.041255
3515.499405	1088281.693496	42.046260
3515.595197	1087978.935374	42.051264
3515.618789	1087698.879809	42.056269
3515.755079	1087399.531965	42.061274
3516.084661	1087100.423264	42.066279
3515.380365	1086805.109842	42.071284
3515.806660	1086489.660820	42.076288
3515.620009	1086206.592125	42.081293
3515.508086	1085921.196135	42.086298
3515.712908	1085618.767770	42.091303
3515.142004	1085320.572075	42.096308
3515.719063	1085022.362676	42.101312
3514.997345	1084737.100820	42.106317
3515.403746	1084435.436239	42.111322
3515.559395	1084151.245467	42.116327
3515.678109	1083862.827227	42.121332
3515.643362	1083569.432962	42.126336
3515.357393	1083282.776562	42.131341
3515.289815	1082980.246382	42.136346
3515.279102	1082684.786672	42.141351
3515.021234	1082409.204095	42.146356
3515.177394	1082098.723836	42.151360
3514.806347	1081826.487289	42.156365
3514.579700	1081535.988426	42.161370
3514.873852	1081242.798298	42.166375
3514.906081	1080979.757826	42.171380
3515.004699	1080691.366767	42.176384
3514.998165	1080405.280346	42.181389
3514.927163	1080123.315193	42.186394
3514.635768	1079834.751156	42.191399
3514.209542	1079550.608015	42.196404
3514.691524	1079278.679409	42.201408
3514.871483	1079000.837141	42.206413
3514.750124	1078713.721222	42.211418
3514.873698	1078429.717043	42.216423
3514.574746	1078142.792276	42.221428
3514.672637	1077861.066264	42.226432
3514.105490	1077587.306448	42.231437
3514.356635	1077302.358677	42.236442
3514.589996	1077027.670990	42.241447
3514.165773	1076766.998487	42.246452
3514.346291	1076483.075650	42.251456
3514.036442	1076209.396363	42.256461
3514.045751	1075941.507970	42.261466
3514.329045	1075674.905652	42.266471
3514.008516	1075399.747196	42.271476
3514.433337	1075117.921837	42.276480
3513.779466	1074855.851453	42.281485
3514.050072	1074581.322733	42.286490
3514.127358	1074311.518415	42.291495
3513.801080	1074055.214595	42.296500
3513.713370	1073783.202175	42.301504
3513.930173	1073523.133797	42.306509
3514.024303	1073246.453769	42.311514
3513.974718	1072982.753044	42.316519
3513.891301	1072714.049233	42.321524
3514.052932	1072445.003624	42.326528
3513.806119	1072171.015617	42.331533
3513.731595	1071901.597845	42.336538
3513.922467	1071635.678611	42.341543
3513.673780	1071383.176672	42.346548
3513.675532	1071105.154295	42.351552
3513.250543	1070843.046051	42.356557
3513.471642	1070582.356661	42.361562
3513.907852	1070344.110983	42.366567
3513.481612	1070070.816338	42.371572
3513.833830	1069806.415784	42.376576
3513.950840	1069543.483187	42.381581
3513.870953	1069271.725869	42.386586
3513.665481	1069008.051602	42.391591
3513.384447	1068741.108142	42.396596
3513.831435	1068489.800406	42.401600
3513.521326	1068238.125075	42.406605
3513.349896	1067956.894494	42.411610
3513.485408	1067700.601602	42.416615
3513.476191	1067446.724781	42.421620
3513.182292	1067174.417889	42.426624
3513.012584	1066933.430921	42.431629
3512.887003	1066678.575937	42.436634
3513.229258	1066427.960443	42.441639
3512.893104	1066173.886188	42.446644
3513.153416	1065913.641636	42.451648
3512.991962	1065662.112184	42.456653
3512.857175	1065398.637502	42.461658
3513.011157	1065151.650512	42.466663
3512.711443	1064907.132458	42.471668
3512.887730	1064647.611443	42.476672
3512.944065	1064414.462670	42.481677
3513.064392	1064177.251987	42.486682
3513.264009	1063903.643028	42.491687
3512.757061	1063664.011504	42.496692
3513.154170	1063405.838984	42.501696
3512.803353	1063162.214051	42.506701
3512.955397	1062905.405797	42.511706
3512.977610	1062654.285819	42.516711
3512.639111	1062409.662972	42.521716
3512.939887	1062153.853941	42.526720
3512.631174	1061905.642101	42.531725
3512.329570	1061657.129074	42.536730
3512.273162	1061419.154572	42.541735
3512.140267	1061181.278650	42.546740
3512.170076	1060934.026258	42.551744
3511.831059	1060714.072578	42.556749
3512.068798	1060466.764945	42.561754
3512.265096	1060231.875056	42.566759
3511.688440	1060009.236083	42.571764
3511.851939	1059766.146336	42.576768
3512.044540	1059541.435687	42.581773
3511.760983	1059309.089430	42.586778
3512.060508	1059066.620575	42.591783
3511.895243	1058848.682650	42.596788
3512.023228	1058604.776934	42.601792
3512.187135	1058377.422794	42.606797
3512.044378	1058148.279489	42.611802
3511.750624	1057917.321152	42.616807
3511.624446	1057683.339015	42.621812
3511.826859	1057456.518570	42.626816
3511.690184	1057229.937334	42.631821
3511.482260	1056997.481092	42.636826
3511.426281	1056772.602085	42.641831
3511.479009	1056545.576100	42.646836
3511.645127	1056310.620312	42.651840
3511.727965	1056108.625770	42.656845
3511.422049	1055859.466199	42.661850
3511.633644	1055641.628458	42.666855
3511.528287	1055426.147408	42.671860
3511.291239	1055198.246274	42.676864
3511.258658	1054977.820204	42.681869
3511.604730	1054751.828710	42.686874
3511.652503	1054530.022053	42.691879
3511.279875	1054316.855158	42.696884
3511.880113	1054075.370397	42.701888
3511.354935	1053859.800912	42.706893
3511.292867	1053636.626759	42.711898
3511.269227	1053401.674751	42.716903
3511.334187	1053193.405922	42.721908
3511.121937	1052968.493978	42.726912
3511.265477	1052747.467721	42.731917
3511.294060	1052536.094481	42.736922
3511.383607	1052318.049241	42.741927
3510.879230	1052095.174934	42.746932
3511.171488	1051870.906698	42.751936
3511.365243	1051667.670493	42.756941
3511.147124	1051446.748210	42.761946
3511.313971	1051225.078528	42.766951
3511.085974	1051009.638163	42.771956
3510.931588	1050788.968456	42.776960
3510.961291	1050576.555477	42.781965
3511.026365	1050358.629887	42.786970
3510.971965	1050140.522444	42.791975
3510.583193	1049945.615368	42.796980
3511.015356	1049722.298152	42.801985
3511.035867	1049515.634632	42.806989
3510.677849	1049304.876857	42.811994
3510.816295	1049094.511728	42.816999
3510.831550	1048875.860498	42.822004
3510.546450	1048650.784803	42.827009
3510.599689	1048457.006927	42.832013
3510.723780	1048246.804942	42.837018
3510.757533	1048041.338728	42.842023
3510.493704	1047839.967366	42.847028
3510.892276	1047611.938001	42.852033
3510.643963	1047399.159260	42.857037
3510.534549	1047204.881751	42.862042
3510.610113	1046998.211675	42.867047
3510.487005	1046798.516719	42.872052
3510.642450	1046584.964488	42.877057
3510.535112	1046391.140756	42.882061
3510.540918	1046176.342447	42.887066
3510.492663	1045962.992873	42.892071
3510.156845	1045749.682444	42.897076
3510.435066	1045543.407458	42.902081
3509.985071	1045348.058850	42.907085
3510.138654	1045142.561911	42.912090
3510.200104	1044937.651900	42.917095
3510.085324	1044744.640853	42.922100
3509.962922	1044538.973866	42.927105
3509.951858	1044345.159281	42.932109
3510.021202	1044149.876047	42.937114
3510.065612	1043958.356617	42.942119
3510.187130	1043769.715335	42.947124
3509.968639	1043570.306075	42.952129
3509.978006	1043381.187126	42.957133
3509.703476	1043179.358319	42.962138
3510.059995	1042993.453116	42.967143
3509.981974	1042805.584682	42.972148
3509.903723	1042605.634654	42.977153
3509.896034	1042406.052223	42.982157
3509.801819	1042210.341235	42.987162
3509.894420	1042008.602594	42.992167
3509.502553	1041822.008518	42.997172
3509.945421	1041630.536347	43.002177
3509.776772	1041441.960347	43.007181
3509.588378	1041245.361246	43.012186
3509.748341	1041054.398939	43.017191
3509.632113	1040866.857696	43.022196
3509.585950	1040688.285702	43.027201
3509.825412	1040496.904597	43.032205
3509.735628	1040303.638281	43.037210
3509.654122	1040108.624257	43.042215
3509.364518	1039925.718785	43.047220
3509.690504	1039734.393819	43.052225
3509.533865	1039557.060140	43.057229
3509.402329	1039370.147477	43.062234
3509.530466	1039180.962538	43.067239
3509.288387	1039003.238611	43.072244
3509.109424	1038810.998381	43.077249
3509.158469	1038630.121190	43.082253
3508.866184	1038454.224733	43.087258
3508.970089	1038279.514266	43.092263
3508.631994	1038096.169851	43.097268
3508.732891	1037930.923631	43.102273
3508.980666	1037766.518489	43.107277
3508.766191	1037584.587144	43.112282
3509.421165	1037407.631364	43.117287
3508.782427	1037237.941820	43.122292
3509.118349	1037047.586434	43.127297
3509.009709	1036873.737115	43.132301
3508.855650	1036706.562484	43.137306
3509.098734	1036514.270054	43.142311
3508.764598	1036361.234086	43.147316
3508.902250	1036175.620368	43.152321
3508.839841	1036005.314726	43.157325
3508.591793	1035830.101727	43.162330
3508.508427	1035666.366128	43.167335
3508.014563	1035500.565355	43.172340
3508.539643	1035322.210537	43.177345
3508.417282	1035163.593206	43.182349
3508.603505	1035006.758488	43.187354
3508.713803	1034822.361715	43.192359
3508.324790	1034672.674171	43.197364
3508.328428	1034504.343286	43.202369
3508.338533	1034332.426645	43.207373
3508.261220	1034170.967989	43.212378
3508.372106	1034010.537926	43.217383
3508.270269	1033848.299946	43.222388
3508.559260	1033692.088580	43.227393
3508.359742	1033534.598657	43.232397
3508.321863	1033363.434106	43.237402
3508.633479	1033204.012163	43.242407
3508.074582	1033036.019869	43.247412
3508.254108	1032867.417032	43.252417
3508.544084	1032710.694154	43.257421
3508.183174	1032548.848114	43.262426
3508.125512	1032388.689467	43.267431
3507.754752	1032227.706742	43.272436
3508.282735	1032069.474908	43.277441
3508.178299	1031918.698641	43.282445
3508.210096	1031749.892778	43.287450
3508.229668	1031596.667609	43.292455
3507.983992	1031427.026532	43.297460
3508.175179	1031274.441824	43.302465
3507.965432	1031111.851581	43.307469
3507.961982	1030961.129601	43.312474
3508.266661	1030800.768878	43.317479
3508.173635	1030638.920090	43.322484
3508.135452	1030487.513369	43.327489
3508.122436	1030325.448686	43.332493
3508.102995	1030163.961268	43.337498
3508.210176	1030005.546602	43.342503
3507.947944	1029837.118587	43.347508
3507.900023	1029688.693349	43.352513
3507.972537	1029546.828715	43.357517
3507.993408	1029384.440648	43.362522
3508.182310	1029225.506235	43.367527
3508.118864	1029075.421065	43.372532
3508.157394	1028904.591287	43.377537
3507.995771	1028759.355804	43.382541
3507.944579	1028599.862079	43.387546
3507.886388	1028444.432580	43.392551
3507.653173	1028297.453608	43.397556
3507.783238	1028132.493040	43.402561
3507.664775	1027993.816588	43.407565
3507.576869	1027840.893449	43.412570
3507.695555	1027694.809252	43.417575
3507.434496	1027539.000532	43.422580
3507.334910	1027390.038400	43.427585
3507.352941	1027244.055867	43.432589
3507.413725	1027096.415663	43.437594
3507.746919	1026957.929734	43.442599
3507.334445	1026826.150779	43.447604
3507.548723	1026662.779866	43.452609
3507.739555	1026514.327843	43.457613
3507.807270	1026375.483692	43.462618
3507.559661	1026219.248431	43.467623
3507.576409	1026074.882661	43.472628
3507.493033	1025930.142088	43.477633
3507.349622	1025782.500827	43.482637
3507.345405	1025642.100008	43.487642
3507.472468	1025496.732180	43.492647
3507.419277	1025351.390265	43.497652
3507.806387	1025197.928990	43.502657
3507.752361	1025071.185565	43.507661
3507.585771	1024911.896331	43.512666
3507.503159	1024770.905107	43.517671
3507.527321	1024611.382078	43.522676
3507.460809	1024469.217626	43.527681
3507.408499	1024326.465706	43.532685
3507.513708	1024185.428799	43.537690
3507.229747	1024029.332200	43.542695
3507.192355	1023896.356243	43.547700
3507.339286	1023737.563510	43.552705
3507.573133	1023603.081970	43.557709
3507.262786	1023471.594862	43.562714
3507.263855	1023325.803669	43.567719
3507.077002	1023190.024384	43.572724
3507.180146	1023039.361958	43.577729
3507.170723	1022900.638177	43.582733
3506.931355	1022767.571736	43.587738
3506.745708	1022616.557716	43.592743
3506.603852	1022494.036164	43.597748
3507.353630	1022361.766685	43.602753
3507.293375	1022225.167530	43.607757
3507.123845	1022082.765539	43.612762
3507.257642	1021943.218797	43.617767
3506.656903	1021810.867870	43.622772
3506.948178	1021676.039729	43.627777
3506.763518	1021543.807895	43.632781
3506.797251	1021413.282432	43.637786
3507.196078	1021272.802620	43.642791
3506.703128	1021156.031005	43.647796
3506.642758	1021018.626661	43.652801
3506.578820	1020874.527969	43.657805
3506.446967	1020755.167064	43.662810
3506.567001	1020616.850329	43.667815
3506.515234	1020496.500889	43.672820
3506.528805	1020375.265214	43.677825
3506.621024	1020246.060776	43.682829
3506.547846	1020119.887368	43.687834
3506.715059	1019987.269884	43.692839
3506.630138	1019863.517508	43.697844
3506.880169	1019731.656318	43.702849
3506.659441	1019601.421586	43.707853
3506.640607	1019477.940824	43.712858
3506.450064	1019350.702404	43.717863
3506.345743	1019223.640913	43.722868
3506.714226	1019088.252813	43.727873
3506.611442	1018964.095498	43.732877
3506.512887	1018833.531778	43.737882
3506.695138	1018705.926294	43.742887
3506.575033	1018582.830581	43.747892
3506.391663	1018451.592812	43.752897
3506.512492	1018325.153043	43.757901
3506.441274	1018194.375905	43.762906
3506.584913	1018063.463306	43.767911
3506.471626	1017944.427639	43.772916
3506.171517	1017809.215845	43.777921
3506.405592	1017699.238799	43.782925
3506.300806	1017593.487961	43.787930
3506.280388	1017467.828439	43.792935
3506.349596	1017344.383273	43.797940
3506.339148	1017214.737791	43.802945
3506.511482	1017097.577980	43.807949
3506.120138	1016979.926284	43.812954
3506.463704	1016842.061972	43.817959
3506.285536	1016733.686705	43.822964
3505.845171	1016609.532908	43.827969
3505.824480	1016491.809937	43.832973
3505.676886	1016380.608222	43.837978
3506.328625	1016271.602069	43.842983
3505.937494	1016160.824350	43.847988
3506.065663	1016035.690682	43.852993
3506.080929	1015922.026494	43.857997
3506.043118	1015808.659950	43.863002
3506.005918	1015693.058435	43.868007
3506.212384	1015579.452899	43.873012
3505.756110	1015455.858642	43.878017
3506.020836	1015338.355718	43.883021
3505.774283	1015236.466849	43.888026
3505.855325	1015112.096997	43.893031
3505.836582	1015007.448246	43.898036
3505.796348	1014891.539505	43.903041
3506.067611	1014781.790488	43.908045
3506.017251	1014683.839755	43.913050
3505.992759	1014558.795443	43.918055
3506.138146	1014441.584706	43.923060
3505.883510	1014324.146133	43.928065
3505.701438	1014201.741332	43.933069
3505.792687	1014096.572041	43.938074
3505.775142	1013978.990113	43.943079
3505.805021	1013870.331155	43.948084
3505.630006	1013765.685033	43.953089
3505.693899	1013668.280406	43.958093
3505.576261	1013556.823676	43.963098
3505.913569	1013443.153439	43.968103
3505.599807	1013332.889867	43.973108
3505.801903	1013232.444536	43.978113
3506.059810	1013117.421241	43.983117
3505.790879	1013002.676597	43.988122
3505.945650	1012884.654957	43.993127
3505.726984	1012777.472589	43.998132
3505.715001	1012678.606541	44.003137
3506.057330	1012561.906938	44.008141
3505.666091	1012452.610099	44.013146
3505.979466	1012334.647932	44.018151
3505.780655	1012235.319235	44.023156
3505.462458	1012124.255674	44.028161
3505.686113	1012014.363397	44.033165
3505.353311	1011913.982640	44.038170
3505.831815	1011800.255983	44.043175
3505.325361	1011697.762976	44.048180
3505.445611	1011589.530783	44.053185
3505.850182	1011485.135345	44.058189
3505.772996	1011388.588777	44.063194
3505.691462	1011277.372383	44.068199
3505.695524	1011156.813576	44.073204
3505.348318	1011033.784162	44.078209
3505.502014	1010952.055902	44.083213
3505.269763	1010856.302951	44.088218
3505.252628	1010744.968284	44.093223
3505.125465	1010649.583127	44.098228
3505.410423	1010546.550185	44.103233
3505.687170	1010435.355314	44.108237
3505.358051	1010343.787465	44.113242
3505.520540	1010235.327977	44.118247
3505.565657	1010135.630570	44.123252
3505.246717	1010031.910365	44.128257
3505.431320	1009934.421254	44.133261
3505.104953	1009836.723106	44.138266
3505.523095	1009731.709938	44.143271
3504.951463	1009629.870211	44.148276
3505.048702	1009527.724126	44.153281
3505.667686	1009436.276897	44.158285
3505.141453	1009334.327172	44.163290
3504.981602	1009225.026728	44.168295
3505.185037	1009137.919042	44.173300
3505.207947	1009047.341139	44.178305
3505.189651	1008953.464274	44.183309
3505.104152	1008855.126321	44.188314
3505.317634	1008755.085205	44.193319
3504.959646	1008665.730168	44.198324
3505.253466	1008567.907873	44.203329
3505.224078	1008466.638149	44.208333
3504.828608	1008368.342758	44.213338
3505.071786	1008273.342357	44.218343
3504.969365	1008177.425293	44.223348
3504.631669	1008087.085753	44.228353
3504.986625	1007992.451014	44.233357
3504.788601	1007913.847088	44.238362
3505.066280	1007812.029021	44.243367
3504.623249	1007721.700975	44.248372
3504.914297	1007642.137855	44.253377
3505.188262	1007536.135488	44.258381
3504.963381	1007441.975858	44.263386
3505.025101	1007351.461537	44.268391
3504.867086	1007252.135446	44.273396
3504.933696	1007156.173175	44.278401
3504.709275	1007073.089936	44.283405
3504.451561	1006988.455452	44.288410
3504.641033	1006898.301698	44.293415
3504.421020	1006804.616727	44.298420
3504.602881	1006719.128027	44.303425
3504.898512	1006624.771804	44.308429
3504.873464	1006559.440358	44.313434
3504.500405	1006454.010368	44.318439
3503.949071	1006377.679470	44.323444
3504.402930	1006286.889031	44.328449
3504.756648	1006213.421012	44.333453
3504.624887	1006138.087325	44.338458
3504.953550	1006058.106755	44.343463
3504.647541	1005963.255159	44.348468
3504.458903	1005869.452259	44.353473
3504.820840	1005783.530784	44.358477
3504.635005	1005688.752022	44.363482
3504.951252	1005596.514536	44.368487
3504.866349	1005526.707819	44.373492
3504.533348	1005432.532458	44.378497
3504.591815	1005343.347914	44.383501
3504.178000	1005267.951820	44.388506
3504.256201	1005175.357670	44.393511
3504.295508	1005105.719790	44.398516
3504.358609	1005025.865598	44.403521
3504.676415	1004933.228017	44.408525
3504.488720	1004851.078556	44.413530
3504.506901	1004770.936392	44.418535
3504.701674	1004686.484628	44.423540
3504.768148	1004595.633565	44.428545
3504.606360	1004509.876245	44.433549
3504.274038	1004433.969280	44.438554
3504.712240	1004338.773289	44.443559
3504.614249	1004258.059397	44.448564
3504.815583	1004176.419646	44.453569
3504.821870	1004095.005378	44.458573
3504.491601	1004011.408153	44.463578
3504.707333	1003921.688914	44.468583
3504.194525	1003843.566487	44.473588
3504.319962	1003749.384818	44.478593
3504.500452	1003676.106899	44.483597
3504.419519	1003598.979994	44.488602
3504.550297	1003502.264117	44.493607
3504.581035	1003422.392597	44.498612
3504.369860	1003346.061935	44.503617
3504.489315	1003254.402330	44.508621
3504.211392	1003184.695741	44.513626
3504.397335	1003101.194593	44.518631
3504.076794	1003025.753189	44.523636
3504.197325	1002948.486939	44.528641
3504.308652	1002869.469931	44.533645
3504.106253	1002813.853347	44.538650
3504.474232	1002714.847245	44.543655
3504.170171	1002636.673740	44.548660
3503.930135	1002554.694091	44.553665
3504.222012	1002480.409380	44.558669
3503.782669	1002404.784659	44.563674
3504.038146	1002336.925718	44.568679
3504.103277	1002260.534885	44.573684
3504.149562	1002191.443749	44.578689
3503.992068	1002112.265834	44.583693
3503.635971	1002041.974205	44.588698
3503.821282	1001979.376954	44.593703
3503.863154	1001908.142369	44.598708
3503.534861	1001841.833234	44.603713
3504.030698	1001766.240558	44.608717
3503.772683	1001698.750464	44.613722
3504.226331	1001621.021977	44.618727
3503.796162	1001555.699380	44.623732
3503.810791	1001487.480671	44.628737
3503.984107	1001405.124333	44.633741
3503.806830	1001346.764352	44.638746
3503.864714	1001269.582804	44.643751
3504.046932	1001208.729254	44.648756
3503.974916	1001135.751969	44.653761
3504.159948	1001064.093900	44.658765
3503.636478	1000996.249858	44.663770
3503.789937	1000917.490613	44.668775
3503.593358	1000853.386631	44.673780
3503.710788	1000790.300788	44.678785
3504.061361	1000718.319101	44.683789
3503.734890	1000655.791505	44.688794
3503.706435	1000574.040274	44.693799
3503.767931	1000513.296462	44.698804
3503.670399	1000446.932962	44.703809
3503.950191	1000374.277240	44.708813
3503.958115	1000313.929443	44.713818
3504.098620	1000254.143177	44.718823
3503.882851	1000184.778694	44.723828
3503.614160	1000112.209946	44.728833
3503.834695	1000038.099611	44.733837
3503.638919	999977.684441	44.738842
3503.792266	999904.654163	44.743847
3503.738252	999833.506596	44.748852
3503.776300	999766.431392	44.753857
3503.515986	999706.023952	44.758861
3503.490688	999635.842614	44.763866
3503.654004	999566.018729	44.768871
3503.632257	999506.153943	44.773876
3503.677766	999441.507355	44.778881
3503.912082	999359.597961	44.783885
3503.545616	999295.212256	44.788890
3503.642169	999229.094565	44.793895
3503.770447	999182.928342	44.798900
3503.734442	999111.963449	44.803905
3503.698234	999034.766930	44.808909
3503.485913	998996.151677	44.813914
3503.911600	998921.214092	44.818919
3503.925389	998857.539642	44.823924
3503.817791	998795.636949	44.828929
3503.497060	998720.819651	44.833933
3503.656841	998658.968787	44.838938
3503.836041	998586.988250	44.843943
3503.503186	998521.711937	44.848948
3503.568466	998459.485002	44.853953
3503.727716	998399.091876	44.858957
3503.602688	998334.168639	44.863962
3503.707875	998275.243616	44.868967
3503.824821	998219.431881	44.873972
3503.499872	998150.352558	44.878977
3503.803367	998083.311075	44.883981
3503.355624	998023.695527	44.888986
3504.001390	997959.322657	44.893991
3503.636124	997886.254404	44.898996
3503.758112	997819.531824	44.904001
3503.524877	997753.743366	44.909005
3503.588730	997694.332222	44.914010
3503.870011	997634.787266	44.919015
3503.995960	997565.334405	44.924020
3503.745250	997487.762611	44.929025
3503.666973	997425.255818	44.934029
3503.468582	997368.805960	44.939034
3503.523792	997293.713119	44.944039
3503.324540	997241.839267	44.949044
3503.283741	997184.679912	44.954049
3503.579027	997123.861246	44.959053
3503.506788	997068.556283	44.964058
3503.569195	997008.066901	44.969063
3503.581694	996951.578152	44.974068
3503.224655	996881.417328	44.979073
3503.588116	996817.370184	44.984077
3503.081596	996764.081656	44.989082
3503.464832	996700.809098	44.994087
3503.656779	996636.982959	44.999092
3503.406287	996584.916738	45.004097
3503.543644	996529.571996	45.009101
3503.354697	996469.605263	45.014106
3503.648739	996395.629993	45.019111
3503.283108	996342.411693	45.024116
3503.315916	996288.835059	45.029121
3503.569599	996229.572110	45.034125
3503.431601	996175.145899	45.039130
3503.440248	996106.181512	45.044135
3503.239006	996047.186396	45.049140
3503.379039	995995.634884	45.054145
3503.495599	995923.728263	45.059149
3503.090637	995873.531724	45.064154
3503.555145	995805.170468	45.069159
3503.712470	995758.484519	45.074164
3503.305704	995696.305001	45.079169
3503.397301	995630.828048	45.084173
3503.306431	995586.422090	45.089178
3503.427164	995515.386343	45.094183
3503.418603	995462.685468	45.099188
3503.238115	995414.103980	45.104193
3503.592579	995339.812743	45.109197
3503.343236	995286.662794	45.114202
3503.153982	995228.144283	45.119207
3503.292394	995170.545423	45.124212
3503.214808	995123.016138	45.129217
3503.310016	995048.471520	45.134221
3503.355837	995001.992563	45.139226
3503.349760	994944.220355	45.144231
3503.616774	994886.012871	45.149236
3503.141678	994828.609015	45.154241
3503.505651	994774.573827	45.159245
3503.468626	994717.583841	45.164250
3503.685079	994652.269895	45.169255
3503.299222	994600.597466	45.174260
3503.674964	994533.307276	45.179265
3503.593932	994462.876188	45.184269
3503.316475	994406.214978	45.189274
3503.542461	994338.557405	45.194279
3503.442279	994295.506987	45.199284
3503.562624	994241.409418	45.204289
3503.571339	994164.821241	45.209293
3503.216415	994122.201222	45.214298
3503.198873	994057.601058	45.219303
3503.326360	994007.397735	45.224308
3503.131436	993947.989972	45.229313
3503.248339	993891.258667	45.234317
3503.262257	993847.991174	45.239322
3503.474596	993783.350027	45.244327
3503.428106	993732.198466	45.249332
3503.029560	993674.575422	45.254337
3503.357644	993616.052524	45.259341
3502.919217	993559.994067	45.264346
3503.304330	993506.625490	45.269351
3503.018247	993449.956150	45.274356
3503.101873	993389.034882	45.279361
3503.167500	993348.191383	45.284365
3503.075027	993299.674743	45.289370
3503.271047	993238.830807	45.294375
3502.882103	993194.455221	45.299380
3503.045102	993139.170655	45.304385
3502.970429	993083.632321	45.309389
3502.840497	993032.683117	45.314394
3502.929436	992981.697407	45.319399
3502.996872	992934.515746	45.324404
3503.022388	992886.755830	45.329409
3503.291901	992834.569522	45.334413
3502.989988	992789.786587	45.339418
3503.047718	992738.998766	45.344423
3503.010581	992697.875126	45.349428
3502.843248	992642.445204	45.354433
3502.792816	992591.381481	45.359437
3502.941487	992551.590709	45.364442
3503.011521	992490.662047	45.369447
3502.597771	992443.653030	45.374452
3502.918025	992389.797309	45.379457
3503.508642	992343.889155	45.384461
3502.965396	992299.824397	45.389466
3503.233096	992252.019257	45.394471
3503.229922	992202.601285	45.399476
3502.782026	992150.429383	45.404481
3503.204301	992093.727308	45.409485
3502.793351	992044.765025	45.414490
3502.630227	992003.559632	45.419495
3502.803485	991953.330621	45.424500
3502.799437	991911.123584	45.429505
3503.018906	991860.203793	45.434509
3503.040976	991817.991762	45.439514
3502.943843	991767.708166	45.444519
3503.057497	991715.244814	45.449524
3502.889928	991658.538068	45.454529
3503.234339	991604.378485	45.459533
3503.002615	991561.816419	45.464538
3503.181487	991495.887473	45.469543
3503.221741	991460.786217	45.474548
3502.940750	991410.139795	45.479553
3503.236794	991356.668227	45.484557
3503.048817	991302.106014	45.489562
3502.970160	991256.201834	45.494567
3502.861790	991202.015505	45.499572
3502.723877	991149.100911	45.504577
3503.105471	991103.022199	45.509581
3502.809766	991063.879158	45.514586
3502.810638	991009.965484	45.519591
3502.874166	990949.411347	45.524596
3502.898713	990904.754760	45.529601
3503.093243	990871.671861	45.534605
3502.982115	990833.764282	45.539610
3502.984475	990768.440955	45.544615
3503.006725	990726.610783	45.549620
3502.979449	990671.528554	45.554625
3503.104594	990614.080679	45.559629
3502.658595	990579.639072	45.564634
3502.914083	990525.483866	45.569639
3503.128553	990474.942506	45.574644
3503.016706	990429.622134	45.579649
3503.256163	990387.656191	45.584653
3502.797662	990335.859374	45.589658
3502.748276	990294.330336	45.594663
3502.928753	990244.280055	45.599668
3502.884426	990199.336753	45.604673
3503.187815	990145.852599	45.609677
3502.613867	990106.456262	45.614682
3502.941514	990052.187160	45.619687
3502.880056	990009.000355	45.624692
3503.003760	989962.564845	45.629697
3502.831002	989911.107139	45.634701
3502.586966	989863.658752	45.639706
3503.141117	989824.269683	45.644711
3503.049536	989772.114751	45.649716
3502.864075	989722.900275	45.654721
3502.990469	989674.024075	45.659725
3502.788006	989631.930313	45.664730
3502.715023	989582.988651	45.669735
3502.811348	989544.355679	45.674740
3503.033571	989493.511771	45.679745
3503.302049	989442.562271	45.684749
3502.836449	989400.217570	45.689754
3502.895644	989343.937987	45.694759
3502.701813	989295.306321	45.699764
3502.698854	989257.662985	45.704769
3503.059954	989212.547588	45.709773
3502.851048	989161.576674	45.714778
3502.871041	989120.222687	45.719783
3503.171910	989066.631285	45.724788
3503.146905	989026.746934	45.729793
3503.058961	988970.390363	45.734797
3502.724427	988934.164899	45.739802
3503.066209	988877.444043	45.744807
3502.828696	988829.595830	45.749812
3502.876509	988781.407626	45.754817
3502.889226	988711.182373	45.759821
3502.625525	988610.473487	45.764826
3502.595116	988443.399206	45.769831
3502.591776	988218.961475	45.774836
3502.575085	987938.233179	45.779841
3502.498036	987594.287534	45.784845
3502.113574	987185.397714	45.789850
3502.541287	986716.926657	45.794855
3502.300233	986174.467170	45.799860
3502.186072	985578.067537	45.804865
3502.041829	984907.241126	45.809869
3501.983995	984176.779345	45.814874
3502.202235	983383.796984	45.819879
3501.880839	982506.921798	45.824884
3501.459325	981566.257439	45.829889
3501.432347	980567.355987	45.834893
3501.038188	979494.681982	45.839898
3501.406861	978328.270334	45.844903
3500.694160	977099.641879	45.849908
3500.466449	975785.917468	45.854913
3500.746634	974396.519481	45.859917
3500.542697	972941.825862	45.864922
3500.228725	971392.279069	45.869927
3500.160452	969772.599645	45.874932
3499.454239	968072.204707	45.879937
3498.983245	966270.806362	45.884941
3498.938158	964428.027288	45.889946
3498.615792	962467.519564	45.894951
3498.690158	960443.451491	45.899956
3498.047552	958326.034867	45.904961
3497.719686	956130.986314	45.909965
3497.153282	953895.225866	45.914970
3496.821998	951589.012273	45.919975
3496.466854	949215.332004	45.924980
3495.985935	946769.708263	45.929985
3495.953532	944235.661458	45.934989
3495.072652	941617.979250	45.939994
3494.330878	938925.587224	45.944999
3494.332777	936155.591253	45.950004
3493.472738	933312.270336	45.955009
3492.708656	930385.078042	45.960013
3492.334982	927392.100163	45.965018
3491.799267	924305.340637	45.970023
3491.609754	921148.816211	45.975028
3490.701248	917922.496242	45.980033
3490.131873	914597.576254	45.985037
3489.681485	911208.151793	45.990042
3489.167038	907718.070243	45.995047
3488.135928	904169.126203	46.000052
3487.573913	900530.925612	46.005057
3487.178527	896809.646138	46.010061
3486.061355	893031.113976	46.015066
3485.532292	889155.241703	46.020071
3485.035129	885213.131883	46.025076
3484.078918	881177.907254	46.030081
3483.289914	877063.649661	46.035085
3482.563157	872882.950466	46.040090
3481.929145	868608.885656	46.045095
3480.952281	864254.962554	46.050100
3480.138685	859837.781433	46.055105
3479.274127	855319.798000	46.060109
3478.225529	850750.035036	46.065114
3477.459651	846091.586501	46.070119
3476.759660	841342.570544	46.075124
3475.660127	836517.980836	46.080129
3474.993185	831601.477180	46.085133
3473.715869	826614.182176	46.090138
3472.898916	821552.032879	46.095143
3472.230329	816410.301947	46.100148
3470.752475	811188.127742	46.105153
3469.890680	805879.007130	46.110157
3468.751315	800496.872789	46.115162
3467.592908	795034.294751	46.120167
3466.834954	789495.100175	46.125172
3465.457157	783866.347115	46.130177
3464.365119	778156.693618	46.135181
3463.118045	772376.970712	46.140186
3461.746570	766504.635765	46.145191
3460.957779	760565.078813	46.150196
3459.604740	754546.940208	46.155201
3458.400041	748446.032555	46.160205
3456.969842	742285.195652	46.165210
3455.700894	736014.846617	46.170215
3454.485630	729672.522912	46.175220
3453.094517	723270.865145	46.180225
3451.688223	716770.939138	46.185229
3450.552341	710199.268057	46.190234
3449.317764	703539.583132	46.195239
3447.507034	696797.120757	46.200244
3446.418947	689970.523522	46.205249
3445.266604	683081.490452	46.210253
3443.939971	676117.135188	46.215258
3442.511357	669055.776801	46.220263
3440.865987	661918.835454	46.225268
3439.182578	654709.866561	46.230273
3437.711751	647411.281539	46.235277
3436.129404	640071.027646	46.240282
3434.993902	632620.548964	46.245287
3433.071172	625098.557731	46.250292
3431.426774	617512.718675	46.255297
3429.938804	609826.017301	46.260301
3428.241378	602092.652002	46.265306
3426.743633	594273.204284	46.270311
3424.868154	586375.470842	46.275316
3422.945811	578403.855156	46.280321
3421.530824	570361.482660	46.285325
3419.249137	562244.708581	46.290330
3417.710683	554055.893648	46.295335
3416.143018	545794.525562	46.300340
3413.638734	537463.045017	46.305345
3411.932669	529051.857212	46.310349
3410.072902	520603.722273	46.315354
3408.142741	512042.054365	46.320359
3406.091322	503421.099395	46.325364
3403.831504	494746.307725	46.330369
3402.206413	485998.493447	46.335373
3400.116155	477186.815123	46.340378
3397.812986	468296.875046	46.345383
3395.319703	459347.039008	46.350388
3393.327067	450338.664855	46.355393
3391.252195	441263.537443	46.360397
3388.737554	432122.837284	46.365402
3386.430432	422933.479659	46.370407
3384.056583	413674.496143	46.375412
3381.705379	404347.825323	46.380417
3379.068378	394959.598364	46.385421
3376.422316	385529.591607	46.390426
3373.642362	376042.461109	46.395431
3371.410652	366506.676903	46.400436
3368.762719	356918.224846	46.405441
3366.487592	347266.086721	46.410445
3363.060616	337587.799893	46.415450
3360.540520	327846.324598	46.420455
3358.068934	318056.737046	46.425460
3354.997151	308223.808500	46.430465
3352.189018	298338.013322	46.435469
3348.783691	288420.773774	46.440474
3345.991449	278447.723899	46.445479
3342.861217	268459.365804	46.450484
3339.386987	258429.353709	46.455489
3336.470464	248358.879801	46.460493
3333.073179	238264.640118	46.465498
3329.207871	228134.612828	46.470503
3326.242061	217889.263184	46.475508
3322.477389	207715.276432	46.480513
3318.680151	197510.820419	46.485517
3314.800632	187303.334011	46.490522
3310.852610	177068.216239	46.495527
3307.008087	166836.476927	46.500532
3302.784172	156588.961594	46.505537
3298.717314	146347.104232	46.510541
3293.818934	136108.621718	46.515546
3289.211321	125862.055495	46.520551
3284.706811	115635.985514	46.525556
3279.036512	105429.228277	46.530561
3274.307041	95232.587730	46.535565
3268.554921	85102.898412	46.540570
3262.671154	74977.504294	46.545575
3256.595873	64903.193973	46.550580
3249.484390	54914.947960	46.555585
3242.048201	44995.258455	46.560589
3232.690469	35212.926307	46.565594
3207.930695	25962.463879	46.570599
3153.648244	17790.578478	46.575604
3095.185313	10343.349749	46.580609
3036.981784	3797.380089	46.585613
2904.642271	427.506561	46.590618
2717.153141	374.742718	46.595623
2632.333644	355.280997	46.600628
2640.098006	356.686664	46.605633
2704.676914	342.820346	46.610637
2782.334401	343.906552	46.615642
2844.577949	338.838116	46.620647
2880.576011	320.946192	46.625652
2891.533458	323.135022	46.630657
2886.432257	325.138040	46.635661
2874.650900	341.285951	46.640666
2863.472971	340.921650	46.645671
2854.916802	325.933213	46.650676
2849.848420	322.717627	46.655681
2847.674417	306.544990	46.660685
2845.868584	311.957625	46.665690
2844.455295	316.143647	46.670695
2842.905021	320.804209	46.675700
2840.087651	324.981767	46.680705
2838.472278	309.274360	46.685709
2835.644115	312.038836	46.690714
2832.017128	312.108439	46.695719
2828.873039	308.720567	46.700724
2825.804825	313.719277	46.705729
2822.607649	309.552767	46.710733
2819.991901	307.033897	46.715738
2816.662905	307.369200	46.720743
2813.577261	292.461232	46.725748
2810.133777	302.409048	46.730753
2807.022400	306.512549	46.735757
2803.748517	299.845670	46.740762
2800.636637	304.704879	46.745767
2797.845350	290.759543	46.750772
2793.871338	305.215807	46.755777
2790.411364	290.016468	46.760781
2787.264691	305.863173	46.765786
2784.303775	300.139972	46.770791
2781.558689	287.997509	46.775796
2777.879810	301.986216	46.780801
2774.340155	284.065714	46.785805
2771.135176	286.848329	46.790810
2767.499574	285.411985	46.795815
2764.189055	285.591245	46.800820
2760.719934	287.985388	46.805825
2757.663525	284.533275	46.810829
2754.224786	281.335694	46.815834
2750.821945	282.610686	46.820839
2747.755355	280.860631	46.825844
2744.248854	281.734997	46.830849
2741.169890	285.744281	46.835853
2736.952723	278.665677	46.840858
2733.385102	280.239547	46.845863
2729.963297	271.035052	46.850868
2726.647572	276.346986	46.855873
2723.653851	271.262223	46.860877
2720.119785	273.498876	46.865882
2717.271797	276.632379	46.870887
2713.799634	267.874239	46.875892
2709.747313	281.382394	46.880897
2706.734433	270.828527	46.885901
2703.271736	268.793761	46.890906
2699.619987	271.371056	46.895911
2696.110925	265.933329	46.900916
2692.808649	270.419361	46.905921
2689.634107	265.661486	46.910925
2685.896168	275.555370	46.915930
2682.460861	264.723398	46.920935
2679.192793	261.066188	46.925940
2675.391939	268.249753	46.930945
2671.821433	267.001619	46.935949
2668.223727	263.575361	46.940954
2665.392050	263.121453	46.945959
2662.323545	261.312853	46.950964
2658.493977	272.428044	46.955969
2655.076800	266.191252	46.960973
2651.534928	263.185550	46.965978
2648.015640	267.437945	46.970983
2644.742773	264.315477	46.975988
2640.957162	265.987978	46.980993
2638.100198	257.081785	46.985997
2633.883252	266.412597	46.991002
2630.652015	243.739248	46.996007
2627.221352	243.925650	47.001012
2623.482423	264.139421	47.006017
2620.673550	262.098606	47.011021
2616.849638	259.414781	47.016026
2612.823807	257.952486	47.021031
2609.836541	254.219708	47.026036
2606.607347	259.081840	47.031041
2603.043343	261.122414	47.036045
2599.628604	259.506781	47.041050
2596.365077	257.278907	47.046055
2592.791450	246.935865	47.051060
2588.657891	260.880882	47.056065
2585.663546	254.335363	47.061069
2582.261095	249.983116	47.066074
2578.568886	252.805392	47.071079
2575.308367	239.753094	47.076084
2571.359358	253.625554	47.081089
2568.354235	245.981987	47.086093
2565.138036	254.113579	47.091098
2560.980178	248.121704	47.096103
2557.916804	243.027594	47.101108
2554.121842	245.013532	47.106113
2550.967620	247.099126	47.111117
2547.160226	236.425980	47.116122
2543.825127	246.698618	47.121127
2540.698988	230.086817	47.126132
2536.940337	249.579500	47.131137
2533.484778	250.632910	47.136141
2530.012818	246.470524	47.141146
2526.189888	240.514112	47.146151
2523.107137	248.358124	47.151156
2519.198079	244.196886	47.156161
2515.813903	249.223317	47.161165
2512.803945	244.396955	47.166170
2509.115213	241.719806	47.171175
2505.663864	236.268626	47.176180
2502.331034	243.391553	47.181185
2498.492590	241.841102	47.186189
2495.035946	238.787392	47.191194
2491.514770	248.244644	47.196199
2488.289085	245.070965	47.201204
2484.455661	236.425322	47.206209
2481.164334	230.592307	47.211213
2477.524442	234.850049	47.216218
2473.829002	243.374228	47.221223
2470.898290	236.855273	47.226228
2467.048458	240.311617	47.231233
2463.949243	237.995937	47.236237
2460.628475	233.623379	47.241242
2456.918979	239.869708	47.246247
2453.519483	233.639391	47.251252
2449.787048	247.135413	47.256257
2446.113782	235.115338	47.261261
2442.763774	228.838490	47.266266
2438.948355	239.774122	47.271271
2435.829814	231.697871	47.276276
2432.201145	237.123467	47.281281
2428.652794	230.035910	47.286285
2425.596415	234.919524	47.291290
2421.793998	235.834050	47.296295
2418.407811	239.160781	47.301300
2415.063548	240.723115	47.306305
2411.208329	224.805223	47.311309
2407.911842	236.983414	47.316314
2404.053501	223.993211	47.321319
2401.089821	225.471477	47.326324
2397.553569	231.806759	47.331329
2394.048295	233.276475	47.336333
2390.147300	232.191504	47.341338
2386.579962	229.709770	47.346343
2383.658429	221.214225	47.351348
2380.134242	221.510774	47.356353
2376.910300	222.943967	47.361357
2373.314807	228.826127	47.366362
2369.731854	228.205583	47.371367
2366.269679	228.179957	47.376372
2362.254910	233.795537	47.381377
2358.633481	224.795660	47.386381
2354.989225	228.374622	47.391386
2351.927331	229.644362	47.396391
2348.719614	225.447868	47.401396
2345.032918	230.034023	47.406401
2341.106731	216.893555	47.411405
2337.893048	217.156081	47.416410
2334.275520	222.637196	47.421415
2331.268930	226.721594	47.426420
2327.430208	226.553076	47.431425
2323.936921	221.954307	47.436429
2320.587587	219.963385	47.441434
2316.789621	219.763388	47.446439
2313.744719	219.470864	47.451444
2309.835293	221.607305	47.456449
2306.351138	223.183679	47.461453
2303.088487	217.473197	47.466458
2299.510982	221.712240	47.471463
2296.235302	213.733413	47.476468
2292.415861	224.707638	47.481473
2289.341956	215.672064	47.486477
2285.632978	216.664183	47.491482
2281.971523	213.781100	47.496487
2278.616756	215.079045	47.501492
2274.842797	220.353548	47.506497
2271.844514	224.135198	47.511501
2268.081696	218.159754	47.516506
2264.632459	213.505411	47.521511
2261.108595	216.032109	47.526516
2257.268845	215.945386	47.531521
2254.050589	217.368221	47.536525
2250.523309	214.847887	47.541530
2246.877048	213.295176	47.546535
2243.701099	208.852773	47.551540
2240.524857	219.992634	47.556545
2237.026097	216.660290	47.561549
2233.413980	201.334053	47.566554
2229.708361	215.178302	47.571559
2226.182033	211.907734	47.576564
2221.915907	217.001894	47.581569
2218.862577	211.082999	47.586573
2215.831200	206.459901	47.591578
2211.972302	210.397427	47.596583
2208.562182	214.167015	47.601588
2205.046531	213.694388	47.606593
2201.806155	215.913702	47.611597
2198.479815	210.222067	47.616602
2194.701812	219.041727	47.621607
2191.089091	216.632495	47.626612
2187.163255	208.807825	47.631617
2183.834736	213.124435	47.636621
2180.557253	209.236885	47.641626
2177.034138	222.083724	47.646631
2173.906540	210.673214	47.651636
2170.599216	212.204696	47.656641
2166.796831	207.754469	47.661645
2163.355682	220.694835	47.666650
2159.697176	216.309175	47.671655
2156.173796	204.417994	47.676660
2152.213270	207.457957	47.681665
2149.183139	211.645352	47.686669
2145.687235	211.585435	47.691674
2142.110273	202.549556	47.696679
2138.546384	206.823219	47.701684
2134.996821	205.837481	47.706689
2131.333144	210.127114	47.711693
2127.794979	202.759449	47.716698
2124.571527	198.511600	47.721703
2121.540679	197.504732	47.726708
2117.848517	207.086097	47.731713
2114.345445	207.893290	47.736717
2110.812085	202.266631	47.741722
2106.778345	213.333689	47.746727
2103.588032	203.635896	47.751732
2100.031935	203.078735	47.756737
2096.785341	207.198165	47.761741
2093.001828	200.291664	47.766746
2089.567888	208.568821	47.771751
2086.329597	203.982774	47.776756
2082.953022	206.256271	47.781761
2079.351087	193.929213	47.786765
2075.567718	205.379007	47.791770
2071.889481	203.082657	47.796775
2068.637212	206.632895	47.801780
2065.213110	207.233520	47.806785
2061.527674	206.934884	47.811789
2058.269508	203.274868	47.816794
2054.544687	203.050707	47.821799
2051.333373	203.721405	47.826804
2047.864408	203.185215	47.831809
2043.800440	212.454626	47.836813
2040.681302	213.125416	47.841818
2036.830433	203.698421	47.846823
2033.732223	203.768492	47.851828
2030.007216	206.388949	47.856833
2026.474144	202.142992	47.861837
2023.160702	193.489027	47.866842
2019.598949	209.083068	47.871847
2016.237354	200.071719	47.876852
2012.348102	203.440263	47.881857
2008.951554	200.933313	47.886861
2005.973984	195.223612	47.891866
2001.962617	203.069128	47.896871
1998.769510	199.560108	47.901876
1995.402012	202.450428	47.906881
1991.549280	201.108998	47.911885
1988.337658	188.773946	47.916890
1984.356211	198.591910	47.921895
1981.347753	196.625127	47.926900
1977.731627	197.022567	47.931905
1974.068880	208.221844	47.936909
1970.476432	193.935147	47.941914
1967.162961	202.643533	47.946919
1963.960874	198.006983	47.951924
1959.967974	195.088580	47.956929
1956.271285	202.833369	47.961933
1953.281842	203.865489	47.966938
1949.622767	202.590297	47.971943
1946.022792	195.295680	47.976948
1942.684781	186.560676	47.981953
1939.122860	203.407606	47.986957
1935.701358	194.184113	47.991962
1932.193976	201.702933	47.996967
1928.803340	185.631622	48.001972
1925.125740	196.913173	48.006977
1921.460743	189.532715	48.011981
1918.098566	189.960112	48.016986
1914.308812	199.517697	48.021991
1911.380281	190.745342	48.026996
1907.739781	200.199382	48.032001
1903.833150	188.612119	48.037005
1900.683456	202.332103	48.042010
1896.821591	196.901627	48.047015
1894.017300	196.746573	48.052020
1889.843790	201.957231	48.057025
1886.412372	200.515175	48.062029
1882.897369	188.834014	48.067034
1879.342003	189.042318	48.072039
1876.440866	185.456482	48.077044
1872.887661	185.568539	48.082049
1869.370985	187.477027	48.087053
1865.795753	189.820487	48.092058
1861.787305	206.033843	48.097063
1858.749839	190.319749	48.102068
1855.173725	189.807151	48.107073
1851.502630	192.738543	48.112077
1847.867494	187.082062	48.117082
1844.424765	196.930580	48.122087
1840.923956	184.627247	48.127092
1837.467847	194.021785	48.132097
1833.786664	191.224381	48.137101
1830.927004	182.848455	48.142106
1827.244732	180.747455	48.147111
1823.742746	180.738913	48.152116
1820.250153	188.892752	48.157121
1816.921332	197.968356	48.162125
1813.286696	188.550330	48.167130
1809.257799	192.501396	48.172135
1805.836905	196.645455	48.177140
1802.171793	199.590584	48.182145
1798.706116	198.876291	48.187149
1795.743877	189.543563	48.192154
1791.842456	189.388138	48.197159
1788.531598	188.881925	48.202164
1785.087021	194.019722	48.207169
1781.593992	190.940417	48.212173
1778.318419	189.510684	48.217178
1774.431401	190.519604	48.222183
1770.966930	181.018975	48.227188
1767.864587	190.445143	48.232193
1764.106704	186.155328	48.237197
1760.583901	179.817293	48.242202
1756.832027	189.994665	48.247207
1753.665481	184.045850	48.252212
1749.747452	184.254468	48.257217
1746.522648	182.619160	48.262221
1743.414286	186.438004	48.267226
1739.416344	193.287754	48.272231
1736.146285	183.371391	48.277236
1732.594361	183.599621	48.282241
1728.938803	182.624178	48.287245
1725.380458	184.947553	48.292250
1721.933275	179.692643	48.297255
1718.244126	181.996563	48.302260
1715.030811	177.529711	48.307265
1711.342449	178.805012	48.312269
1708.410359	188.910374	48.317274
1704.430789	189.241442	48.322279
1700.946057	179.598877	48.327284
1697.299744	190.458131	48.332289
1693.678873	190.478641	48.337293
1690.807557	180.225599	48.342298
1686.987268	181.884256	48.347303
1683.953696	187.123964	48.352308
1679.667366	179.715754	48.357313
1676.137775	185.343738	48.362317
1673.106770	175.051452	48.367322
1669.556162	176.699161	48.372327
1666.463320	173.374233	48.377332
1662.610832	177.636528	48.382337
1658.652725	174.276503	48.387341
1655.532269	173.737456	48.392346
1651.823112	183.318543	48.397351
1648.391340	171.241217	48.402356
1644.787261	183.103562	48.407361
1641.421383	184.844813	48.412365
1637.941056	172.635807	48.417370
1634.373688	184.360688	48.422375
1631.234166	171.720160	48.427380
1627.588024	176.072432	48.432385
1623.845616	175.768822	48.437389
1620.423562	160.274339	48.442394
1616.443447	178.135380	48.447399
1613.479215	164.488654	48.452404
1609.830114	183.139084	48.457409
1606.321032	179.066192	48.462413
1602.922495	170.410928	48.467418
1599.302020	177.470939	48.472423
1596.075141	176.285227	48.477428
1592.701826	175.204185	48.482433
1589.034147	180.196363	48.487437
1585.483598	170.301026	48.492442
1581.236054	181.175974	48.497447
1578.594852	166.372488	48.502452
1575.189363	176.839345	48.507457
1571.459485	175.874868	48.512461
1568.217770	174.985120	48.517466
1564.006591	180.008793	48.522471
1560.356207	169.288310	48.527476
1557.297807	174.502955	48.532481
1553.739604	175.326616	48.537485
1550.435660	172.817838	48.542490
1546.289180	177.138572	48.547495
1543.432707	171.261527	48.552500
1540.049376	176.871942	48.557505
1536.665751	174.091697	48.562509
1533.285763	171.903975	48.567514
1529.291755	181.442739	48.572519
1525.652696	168.349208	48.577524
1522.343916	171.662745	48.582529
1518.776259	167.645643	48.587533
1515.482720	162.732102	48.592538
1511.637070	175.961875	48.597543
1508.244937	176.691459	48.602548
1504.709700	174.935244	48.607553
1501.528781	172.487677	48.612557
1497.858544	172.159694	48.617562
1494.408822	174.946792	48.622567
1491.249371	171.207535	48.627572
1487.386288	165.869366	48.632577
1483.681859	180.047314	48.637581
1480.292642	169.248954	48.642586
1476.599350	179.792155	48.647591
1473.362390	165.208198	48.652596
1469.714667	173.795518	48.657601
1466.491226	171.484817	48.662605
1462.970826	177.136434	48.667610
1459.187057	181.562407	48.672615
1455.868073	172.703295	48.677620
1452.328639	177.016334	48.682625
1448.796472	167.581732	48.687629
1445.260175	177.445141	48.692634
1441.511887	175.544073	48.697639
1438.306893	163.050320	48.702644
1434.570414	166.648862	48.707649
1431.280961	170.434574	48.712653
1428.143962	166.341315	48.717658
1424.526010	165.773394	48.722663
1420.418131	169.834672	48.727668
1417.314177	167.259707	48.732673
1413.781881	168.485920	48.737677
1410.513486	158.545511	48.742682
1406.839856	168.968975	48.747687
1403.468534	168.414027	48.752692
1399.660919	167.977656	48.757697
1395.865081	169.239680	48.762701
1392.631769	175.212029	48.767706
1389.106699	165.413436	48.772711
1385.737188	168.820420	48.777716
1382.073534	168.473851	48.782721
1378.624450	169.923417	48.787725
1375.325922	165.187169	48.792730
1371.668892	172.245715	48.797735
1368.535970	165.194699	48.802740
1364.769670	171.881888	48.807745
1361.093864	175.564967	48.812749
1358.095449	168.996477	48.817754
1354.139031	175.355255	48.822759
1350.913372	167.074613	48.827764
1347.061778	176.137714	48.832769
1343.591804	166.423383	48.837773
1340.526880	168.541686	48.842778
1336.597633	162.428243	48.847783
1333.104448	173.848670	48.852788
1329.683225	169.905172	48.857793
1326.112405	169.300122	48.862797
1322.775846	169.589200	48.867802
1318.980832	168.745811	48.872807
1315.579958	166.194648	48.877812
1311.806496	166.153034	48.882817
1308.691055	170.358368	48.887821
1305.641960	169.285119	48.892826
1301.802088	160.840704	48.897831
1298.417052	162.169143	48.902836
1294.634786	163.890295	48.907841
1291.033424	167.805785	48.912845
1287.734874	159.449806	48.917850
1283.727928	169.075756	48.922855
1280.399231	175.593775	48.927860
1277.161072	166.310329	48.932865
1273.358960	162.457457	48.937869
1270.589049	163.763693	48.942874
1266.615475	172.364734	48.947879
1263.314811	171.433856	48.952884
1259.610993	165.812144	48.957889
1255.875482	176.760282	48.962893
1252.809670	157.763162	48.967898
1249.381622	176.135503	48.972903
1245.827169	161.316123	48.977908
1242.061956	166.088280	48.982913
1238.370388	169.463056	48.987917
1234.824034	164.684624	48.992922
1231.338417	174.506011	48.997927
1227.879332	169.027418	49.002932
1225.043524	158.121492	49.007937
1221.386352	170.211474	49.012941
1217.607968	161.741079	49.017946
1214.306083	167.647175	49.022951
1210.492508	167.720167	49.027956
1207.128933	164.734244	49.032961
1203.065641	167.781993	49.037965
1200.124779	167.559194	49.042970
1196.512773	165.916839	49.047975
1193.366439	165.416211	49.052980
1189.446502	167.457395	49.057985
1185.665271	166.333102	49.062989
1182.821979	164.801519	49.067994
1178.911159	165.370542	49.072999
1175.518146	163.213370	49.078004
1172.064772	168.582844	49.083009
1168.576714	169.378050	49.088013
1165.109748	162.382978	49.093018
1161.497994	157.886886	49.098023
1158.288733	163.363556	49.103028
1154.605129	155.751155	49.108033
1150.801822	163.116792	49.113037
1147.783067	161.418062	49.118042
1143.878743	161.592692	49.123047
1140.480695	158.817503	49.128052
1136.989558	158.048358	49.133057
1133.387134	156.691643	49.138061
1130.152915	146.832678	49.143066
1126.425123	149.356170	49.148071
1123.188955	155.112839	49.153076
1119.381146	159.287032	49.158081
1115.728518	154.072399	49.163085
1112.495182	157.279049	49.168090
1109.202623	162.767912	49.173095
1105.753613	154.530502	49.178100
1102.198870	154.455658	49.183105
1098.149218	155.647769	49.188109
1095.173937	158.696792	49.193114
1091.383535	155.903335	49.198119
1087.922726	150.458360	49.203124
1084.569905	163.711315	49.208129
1080.810831	176.459148	49.213133
1077.544346	154.506303	49.218138
1073.486872	167.674243	49.223143
1070.258629	157.645124	49.228148
1066.852766	164.246900	49.233153
1063.373709	176.715289	49.238157
1060.295289	152.956200	49.243162
1056.185859	163.314725	49.248167
1053.048978	156.252597	49.253172
1049.765392	156.320952	49.258177
1045.886289	150.804377	49.263181
1042.629677	147.843110	49.268186
1039.037356	155.940713	49.273191
1035.319905	158.304993	49.278196
1031.910530	166.332149	49.283201
1028.185680	159.383582	49.288205
1024.794922	151.876029	49.293210
1021.069305	157.333824	49.298215
1017.545530	159.375104	49.303220
1014.304102	160.247267	49.308225
1011.128593	159.115903	49.313229
1007.720844	154.042529	49.318234
1004.307201	157.597456	49.323239
1000.972358	157.325648	49.328244
997.051585	164.774978	49.333249
993.206775	168.701703	49.338253
989.613064	167.549028	49.343258
986.038658	171.910875	49.348263
982.811449	159.023583	49.353268
979.523152	157.098034	49.358273
975.791587	164.158607	49.363277
972.300201	152.250989	49.368282
968.677474	158.963492	49.373287
965.513841	158.438893	49.378292
962.167103	157.916807	49.383297
958.451572	159.565164	49.388301
954.976257	165.708955	49.393306
951.175187	160.128844	49.398311
947.556274	149.656034	49.403316
944.430905	162.947348	49.408321
940.835489	162.014588	49.413325
937.672649	159.674216	49.418330
933.705742	155.625207	49.423335
929.931196	159.980859	49.428340
926.844858	151.093321	49.433345
923.219911	158.474108	49.438349
920.091743	154.390108	49.443354
916.209639	156.023964	49.448359
912.905775	150.701552	49.453364
909.552767	147.201037	49.458369
905.632211	159.548120	49.463373
902.113569	154.549645	49.468378
898.669326	156.672463	49.473383
895.403151	150.112224	49.478388
891.993624	151.102174	49.483393
888.127503	163.927341	49.488397
884.739077	150.193539	49.493402
881.180235	156.754160	49.498407
877.975012	156.443647	49.503412
874.378723	154.780229	49.508417
870.373326	163.148265	49.513421
867.362917	146.049865	49.518426
863.820089	163.826937	49.523431
860.160337	151.736071	49.528436
856.954443	152.858845	49.533441
853.117841	160.681075	49.538445
849.884918	147.192726	49.543450
846.044652	157.103701	49.548455
842.657806	151.922690	49.553460
839.524453	159.783492	49.558465
835.612977	161.280378	49.563469
832.422238	157.790793	49.568474
828.705804	160.913871	49.573479
825.044078	159.986995	49.578484
821.888079	160.058266	49.583489
818.198519	157.821605	49.588493
814.568613	154.639153	49.593498
811.412002	160.259497	49.598503
807.736052	159.259903	49.603508
804.215278	162.776283	49.608513
800.428088	159.792853	49.613517
797.358561	158.341811	49.618522
793.625316	151.912525	49.623527
790.227245	159.484493	49.628532
786.774980	163.814525	49.633537
783.013839	157.828570	49.638541
779.784829	152.893127	49.643546
775.984780	155.091040	49.648551
772.548645	162.386951	49.653556
769.348962	158.278038	49.658561
765.632105	155.864587	49.663565
762.156083	147.935805	49.668570
758.101989	164.483158	49.673575
754.953276	160.310884	49.678580
751.834122	149.978237	49.683585
748.487197	152.578431	49.688589
745.045105	150.603029	49.693594
741.037027	158.724834	49.698599
737.909649	150.630068	49.703604
734.019345	147.231303	49.708609
729.943518	157.706474	49.713613
727.076354	157.553498	49.718618
723.843712	155.825572	49.723623
720.189367	156.493284	49.728628
716.698053	141.788560	49.733633
712.800513	156.007262	49.738637
709.804535	143.533709	49.743642
706.167648	163.789687	49.748647
702.700842	149.140900	49.753652
699.066610	145.206592	49.758657
695.527899	155.434141	49.763661
692.341778	147.993124	49.768666
688.428921	148.511465	49.773671
684.898175	150.846872	49.778676
681.830106	147.675298	49.783681
678.141297	156.297665	49.788685
674.869109	144.902865	49.793690
671.235964	150.468781	49.798695
667.456043	146.111645	49.803700
664.159203	148.774343	49.808705
660.279011	146.016199	49.813709
656.697202	145.523620	49.818714
653.322604	155.402271	49.823719
650.242742	151.516029	49.828724
646.739225	159.181636	49.833729
643.122406	151.327282	49.838733
639.571103	148.316042	49.843738
635.850532	147.992205	49.848743
632.417605	151.207172	49.853748
629.243094	158.890565	49.858753
625.617544	152.135005	49.863757
622.284702	151.005055	49.868762
618.323381	152.062205	49.873767
614.994699	147.245622	49.878772
611.419914	155.006475	49.883777
608.178808	145.906430	49.888781
604.727235	147.066249	49.893786
600.876581	146.799532	49.898791
597.394053	151.116201	49.903796
594.044841	145.920041	49.908801
590.468044	144.380731	49.913805
587.284708	151.185000	49.918810
583.301651	153.006590	49.923815
579.889567	149.948317	49.928820
576.601749	143.528079	49.933825
572.976334	150.257881	49.938829
569.525553	149.507233	49.943834
565.920270	152.425336	49.948839
562.336930	154.294568	49.953844
558.857504	149.299980	49.958849
555.090928	152.787530	49.963853
552.061039	146.069283	49.968858
548.637530	158.521777	49.973863
545.177468	158.125760	49.978868
541.261248	139.532711	49.983873
537.679175	153.562448	49.988877
534.420235	144.692299	49.993882
530.906490	157.897643	49.998887
527.417433	152.727774	50.003892
523.984582	152.800029	50.008897
520.441128	160.335851	50.013901
517.369246	153.525802	50.018906
513.845075	147.763401	50.023911
509.668656	157.715362	50.028916
506.439397	144.761437	50.033921
502.757354	147.289739	50.038925
499.279348	148.844653	50.043930
495.721775	148.064034	50.048935
492.408901	140.805175	50.053940
489.075748	142.078875	50.058945
484.973709	142.854406	50.063949
482.029838	141.065588	50.068954
478.485388	149.960066	50.073959
475.061624	148.951265	50.078964
471.581738	148.580859	50.083969
467.965900	146.994201	50.088973
464.496830	144.399713	50.093978
460.774927	141.171996	50.098983
457.210162	141.421359	50.103988
453.920527	143.031306	50.108993
449.925859	142.536996	50.113997
446.771820	143.465829	50.119002
443.425853	141.755881	50.124007
440.132341	145.947975	50.129012
436.679329	134.455148	50.134017
432.391251	140.703242	50.139021
429.316529	144.726015	50.144026
425.801857	146.035849	50.149031
421.964261	142.557840	50.154036
419.093810	135.651834	50.159041
415.461031	149.369858	50.164045
412.003223	148.453531	50.169050
408.415066	140.306626	50.174055
404.810901	140.819621	50.179060
401.417775	136.139987	50.184065
397.670225	146.416956	50.189069
394.257860	145.137778	50.194074
390.768394	136.418072	50.199079
387.356010	139.380858	50.204084
383.931217	128.874987	50.209089
380.098826	139.108657	50.214093
376.566815	135.351613	50.219098
373.069635	140.784720	50.224103
369.834603	143.162791	50.229108
366.729586	137.082038	50.234113
362.856556	150.019656	50.239117
359.161689	143.905926	50.244122
355.061431	145.518627	50.249127
351.505748	143.313597	50.254132
348.720376	138.894567	50.259137
345.354027	151.389782	50.264141
341.758843	140.444159	50.269146
338.417370	148.136898	50.274151
335.035718	133.657120	50.279156
331.235233	142.685707	50.284161
327.820827	138.636186	50.289165
324.325672	133.200790	50.294170
320.649553	138.219833	50.299175
317.112579	138.217651	50.304180
313.945958	132.881886	50.309185
310.551455	147.250774	50.314189
306.933283	139.238920	50.319194
303.194801	137.913930	50.324199
299.622394	138.320221	50.329204
296.080835	126.057127	50.334209
292.608618	142.583805	50.339213
288.853936	140.806800	50.344218
285.725436	149.291497	50.349223
282.222641	139.429764	50.354228
278.826166	135.789094	50.359233
275.098357	149.485190	50.364237
271.743443	139.137624	50.369242
268.042875	148.465137	50.374247
264.690685	142.206754	50.379252
261.167728	137.119010	50.384257
257.610571	139.280633	50.389261
254.373697	132.355245	50.394266
250.949762	138.807249	50.399271
247.078078	141.945434	50.404276
243.728417	135.997213	50.409281
240.093935	137.375380	50.414285
236.664691	134.206785	50.419290
233.247057	133.727274	50.424295
229.646604	130.473419	50.429300
226.288590	130.652545	50.434305
222.166001	132.139878	50.439309
218.882303	129.289084	50.444314
215.729260	133.979363	50.449319
212.342436	139.798403	50.454324
209.197940	131.719897	50.459329
205.283037	139.169148	50.464333
201.538943	135.286048	50.469338
198.188056	138.784524	50.474343
194.314969	136.084103	50.479348
191.201843	130.118538	50.484353
187.429794	140.243086	50.489357
184.127381	135.862805	50.494362
180.415521	135.860097	50.499367
177.019116	133.081616	50.504372
173.834422	129.749136	50.509377
169.917368	132.876707	50.514381
166.473511	135.728293	50.519386
163.182237	132.368343	50.524391
159.462477	133.979855	50.529396
156.123045	127.289894	50.534401
152.732354	131.626625	50.539405
149.107887	126.989213	50.544410
145.218474	138.702271	50.549415
141.888234	136.910175	50.554420
138.620055	139.119412	50.559425
135.138497	137.798044	50.564429
131.864505	132.689170	50.569434
127.668861	128.931439	50.574439
124.149492	144.753490	50.579444
121.445646	139.519531	50.584449
117.580744	132.166151	50.589453
114.389415	131.602647	50.594458
110.477241	129.075465	50.599463
106.985773	134.996490	50.604468
103.629772	123.446033	50.609473
99.743690	131.035301	50.614477
96.589573	124.670108	50.619482
92.959948	134.130503	50.624487
89.613311	140.965415	50.629492
86.227009	126.411211	50.634497
82.350838	134.299155	50.639501
78.911273	130.598045	50.644506
75.671270	132.091162	50.649511
72.041869	132.766360	50.654516
68.431708	130.321200	50.659521
64.756274	138.593194	50.664525
61.629238	130.886678	50.669530
57.882687	136.126347	50.674535
54.596797	137.053876	50.679540
51.301026	131.135933	50.684545
47.125855	145.739780	50.689549
44.194091	126.706758	50.694554
40.550939	134.677366	50.699559
36.885476	138.826540	50.704564
33.637360	138.467796	50.709569
29.863350	134.749668	50.714573
26.473195	132.470516	50.719578
23.171167	136.697557	50.724583
19.138367	131.406046	50.729588
15.726558	128.200071	50.734593
12.452849	134.450375	50.739597
9.025586	139.830375	50.744602
5.512517	128.854946	50.749607
1.985418	135.728399	50.754612