Thu Jun 16 10:45:55 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
-0.089445	85.764821	0.000000
-0.071497	86.890916	0.005005
-0.461487	103.269146	0.010010
-0.491441	84.709461	0.015014
-0.505536	80.659352	0.020019
-0.776207	70.079525	0.025024
-1.364044	58.106052	0.030029
-1.365136	53.541986	0.035034
-1.871388	50.357317	0.040038
-2.153605	50.079450	0.045043
-2.429229	43.009177	0.050048
-2.657458	37.685334	0.055053
-2.785343	35.429905	0.060058
-2.883574	29.817131	0.065062
-3.133040	30.607598	0.070067
-3.994772	25.733539	0.075072
-4.028149	22.276580	0.080077
-4.255616	27.473716	0.085082
-4.350656	29.019506	0.090086
-4.584659	24.133459	0.095091
-5.180532	33.631311	0.100096
-5.497461	16.717618	0.105101
-5.822374	32.211539	0.110106
-5.705070	28.944743	0.115110
-5.673914	29.246868	0.120115
-5.903832	34.962047	0.125120
-6.677850	24.328995	0.130125
-6.935334	26.082462	0.135130
-7.387932	26.215528	0.140134
-7.172562	20.828840	0.145139
-7.718459	29.611875	0.150144
-7.498854	32.198749	0.155149
-8.120144	27.456514	0.160154
-8.680589	23.426862	0.165158
-9.011364	19.828749	0.170163
-8.997782	31.406716	0.175168
-8.920717	26.107205	0.180173
-8.795470	37.985177	0.185178
-9.288496	26.147891	0.190182
-10.117708	16.661048	0.195187
-10.587166	30.359487	0.200192
-10.482133	21.857895	0.205197
-10.606083	26.918751	0.210202
-10.540052	28.903173	0.215206
-10.412278	22.720324	0.220211
-11.270595	22.162583	0.225216
-11.576149	16.653528	0.230221
-11.806825	24.969531	0.235226
-12.016342	25.849288	0.240230
-11.998507	19.950085	0.245235
-12.433791	26.489117	0.250240
-12.764474	23.562523	0.255245
-13.128041	28.089209	0.260250
-13.364152	17.620020	0.265254
-13.297800	22.153988	0.270259
-13.837532	20.825106	0.275264
-14.727870	22.441948	0.280269
-14.845974	27.925160	0.285274
-14.654487	19.697844	0.290278
-14.543142	22.733525	0.295283
-14.906887	30.733831	0.300288
-15.257454	20.846374	0.305293
-15.231390	21.505677	0.310298
-16.032679	29.393709	0.315302
-16.463395	19.432979	0.320307
-16.869525	28.663098	0.325312
-16.445692	26.863233	0.330317
-16.802735	23.755329	0.335322
-16.915973	21.388273	0.340326
-16.845264	31.309878	0.345331
-17.649612	25.936326	0.350336
-18.161917	16.648186	0.355341
-18.006753	28.914045	0.360346
-18.098809	29.150012	0.365350
-18.307797	26.521759	0.370355
-18.861843	28.038634	0.375360
-19.128324	18.030541	0.380365
-19.492471	29.373094	0.385370
-19.548302	30.683824	0.390374
-19.855743	21.501223	0.395379
-20.313270	32.673052	0.400384
-19.956703	18.939140	0.405389
-20.484561	29.390778	0.410394
-21.243576	23.467240	0.415398
-21.209043	20.406597	0.420403
-21.429420	23.849883	0.425408
-21.138318	28.080839	0.430413
-21.518880	18.093769	0.435418
-22.159880	21.870662	0.440422
-22.393776	15.740384	0.445427
-23.003408	16.921157	0.450432
-22.722869	16.047948	0.455437
-23.243967	17.868951	0.460442
-23.095488	25.227409	0.465446
-23.659092	16.628260	0.470451
-24.258589	24.202569	0.475456
-24.419906	22.743079	0.480461
-24.621264	36.547171	0.485466
-24.697012	37.020566	0.490470
-24.375222	28.800814	0.495475
-24.564551	16.224255	0.500480
-25.010182	19.781913	0.505485
-25.940684	30.222353	0.510490
-26.353600	26.746530	0.515494
-26.169086	25.067998	0.520499
-26.316299	34.058123	0.525504
-26.088398	32.031474	0.530509
-27.065248	28.289748	0.535514
-27.662869	33.679365	0.540518
-27.907865	24.395190	0.545523
-27.814066	19.949030	0.550528
-28.070164	13.576677	0.555533
-28.198426	34.463249	0.560538
-28.236833	24.087170	0.565542
-27.904990	31.162873	0.570547
-28.239911	32.944824	0.575552
-28.974097	27.025371	0.580557
-29.280045	22.322775	0.585562
-29.595339	21.229679	0.590566
-29.646365	13.346298	0.595571
-30.444040	32.009847	0.600576
-30.756423	26.669433	0.605581
-31.174882	19.138687	0.610586
-31.029881	22.483411	0.615590
-31.239658	20.915915	0.620595
-31.478971	27.169910	0.625600
-31.194750	19.099124	0.630605
-31.390960	27.831570	0.635610
-32.489616	28.672601	0.640614
-32.606909	26.710299	0.645619
-33.164380	26.292850	0.650624
-32.803935	19.753197	0.655629
-33.201685	28.336145	0.660634
-33.264180	14.650282	0.665638
-33.135663	23.304397	0.670643
-33.770998	36.148390	0.675648
-34.269293	30.648495	0.680653
-34.500867	27.580923	0.685658
-34.833987	20.259820	0.690662
-34.802631	22.328696	0.695667
-34.881965	28.722681	0.700672
-35.093796	16.365894	0.705677
-35.565556	22.464348	0.710682
-36.185925	31.032887	0.715686
-36.288237	23.960917	0.720691
-36.475257	28.370823	0.725696
-36.428458	25.746371	0.730701
-36.600166	27.099928	0.735706
-37.451588	23.969845	0.740710
-37.534171	25.216234	0.745715
-37.835553	22.892801	0.750720
-37.746119	23.772085	0.755725
-37.675379	24.520783	0.760730
-38.272255	19.725785	0.765734
-38.771979	21.527670	0.770739
-38.965085	31.645390	0.775744
-39.126133	30.599609	0.780749
-39.448372	28.546085	0.785754
-39.115264	22.800275	0.790758
-39.359894	31.692355	0.795763
-40.242179	28.026258	0.800768
-40.504223	35.487782	0.805773
-40.505048	29.242231	0.810778
-40.485290	33.056528	0.815782
-41.064238	16.140074	0.820787
-41.605043	33.198108	0.825792
-41.999339	23.629922	0.830797
-42.174743	24.516768	0.835802
-42.507870	35.453073	0.840806
-41.913714	31.913814	0.845811
-42.631945	34.204039	0.850816
-43.578280	29.133244	0.855821
-43.608800	36.547135	0.860826
-43.405158	27.441468	0.865830
-43.466702	23.350977	0.870835
-43.872741	30.622119	0.875840
-43.846890	30.000342	0.880845
-43.914538	26.206326	0.885850
-44.801569	25.930650	0.890854
-45.073526	22.524466	0.895859
-45.270852	27.856906	0.900864
-45.300336	25.388800	0.905869
-45.866078	38.047169	0.910874
-45.849964	26.918725	0.915878
-46.113466	32.127243	0.920883
-46.585925	31.018785	0.925888
-46.663967	25.071993	0.930893
-46.797078	29.986185	0.935898
-47.038393	31.312869	0.940902
-47.218297	41.264747	0.945907
-47.556996	29.645142	0.950912
-48.314033	33.860592	0.955917
-48.893605	30.081133	0.960922
-48.914470	37.574620	0.965926
-48.657507	31.115005	0.970931
-48.632988	35.066433	0.975936
-48.837904	34.321298	0.980941
-49.068441	32.430689	0.985946
-49.229046	37.762884	0.990950
-49.789339	22.680665	0.995955
-50.375918	34.321412	1.000960
-50.365307	30.253030	1.005965
-50.399070	31.392402	1.010970
-50.946873	32.241448	1.015974
-51.524248	29.943106	1.020979
-51.802611	27.627609	1.025984
-51.965649	29.936277	1.030989
-52.222921	27.316697	1.035994
-52.240079	27.596223	1.040998
-52.024277	31.062232	1.046003
-52.459243	30.399806	1.051008
-52.722282	21.813236	1.056013
-53.120556	27.263727	1.061018
-53.468545	31.976071	1.066022
-53.594537	28.990790	1.071027
-54.188742	23.752299	1.076032
-54.049419	25.758445	1.081037
-54.459505	23.534662	1.086042
-55.295717	30.745786	1.091046
-54.967153	22.247408	1.096051
-55.309761	33.198891	1.101056
-55.186297	25.026225	1.106061
-55.143125	34.922388	1.111066
-55.651942	28.197084	1.116070
-55.973069	40.814240	1.121075
-56.522173	40.463875	1.126080
-56.797117	34.900038	1.131085
-56.839066	37.254794	1.136090
-57.257036	35.156814	1.141094
-57.503404	22.104208	1.146099
-58.354470	35.220423	1.151104
-58.345003	35.440500	1.156109
-58.246585	28.767755	1.161114
-58.647352	27.145206	1.166118
-58.782080	28.129113	1.171123
-58.646838	27.362784	1.176128
-58.743337	28.928743	1.181133
-59.492212	30.763026	1.186138
-59.946572	28.505027	1.191142
-59.975791	16.687393	1.196147
-60.165964	30.390677	1.201152
-60.240389	21.530250	1.206157
-59.968170	16.545850	1.211162
-61.249012	21.650410	1.216166
-61.238497	14.209779	1.221171
-61.896130	24.233098	1.226176
-61.724161	21.844066	1.231181
-62.013871	21.082658	1.236186
-62.005163	26.929067	1.241190
-61.819505	26.496536	1.246195
-62.728563	38.638269	1.251200
-62.897301	30.416816	1.256205
-63.040099	26.370434	1.261210
-63.180101	30.236585	1.266214
-64.051657	23.930924	1.271219
-64.678621	33.217369	1.276224
-64.714437	26.921864	1.281229
-64.316789	33.606478	1.286234
-64.517877	32.204270	1.291238
-64.674125	32.235585	1.296243
-65.009268	37.341507	1.301248
-65.355897	25.324955	1.306253
-65.806521	22.865186	1.311258
-66.379701	19.722174	1.316262
-66.108306	16.292195	1.321267
-66.813865	21.916686	1.326272
-66.869351	30.719694	1.331277
-66.899294	28.954076	1.336282
-66.942067	31.601869	1.341286
-66.973813	25.215325	1.346291
-67.894099	25.959108	1.351296
-68.434663	29.673434	1.356301
-67.950642	26.633707	1.361306
-68.452173	30.027667	1.366310
-68.376386	28.863528	1.371315
-69.089048	31.837786	1.376320
-69.519903	31.087669	1.381325
-69.936497	27.272894	1.386330
-70.181185	33.120734	1.391334
-70.025458	29.754065	1.396339
-70.337356	30.664653	1.401344
-70.205693	26.354987	1.406349
-70.096526	29.279549	1.411354
-70.875094	31.744894	1.416358
-71.087083	18.099525	1.421363
-71.352790	34.380776	1.426368
-71.803895	31.714308	1.431373
-71.491859	28.390864	1.436378
-72.868728	32.393457	1.441382
-73.073839	27.832537	1.446387
-73.267565	31.275169	1.451392
-73.029943	35.204596	1.456397
-72.906820	22.415400	1.461402
-73.327580	27.482294	1.466406
-73.264682	18.991717	1.471411
-73.947959	32.457252	1.476416
-74.491538	22.547443	1.481421
-74.504414	24.972270	1.486426
-74.901299	35.429098	1.491430
-74.799447	26.415332	1.496435
-74.882458	33.452257	1.501440
-75.292335	22.356636	1.506445
-75.843248	29.639487	1.511450
-76.433624	27.350499	1.516454
-76.542993	19.982755	1.521459
-76.822074	31.285597	1.526464
-76.632494	23.287770	1.531469
-76.409849	26.246060	1.536474
-76.967442	34.065705	1.541478
-77.616755	21.026919	1.546483
-78.146615	39.256334	1.551488
-77.881322	23.947016	1.556493
-78.009993	26.325375	1.561498
-78.389188	26.293206	1.566502
-78.469726	30.226380	1.571507
-79.604385	29.821456	1.576512
-79.609692	32.606598	1.581517
-79.869606	24.786052	1.586522
-80.221847	22.918223	1.591526
-80.094150	27.804404	1.596531
-80.199171	23.762238	1.601536
-79.980496	28.893039	1.606541
-80.036855	25.280457	1.611546
-80.948181	25.663170	1.616550
-81.350918	28.066699	1.621555
-81.725874	29.934684	1.626560
-81.433372	26.772116	1.631565
-81.171693	22.044082	1.636570
-82.341238	32.011230	1.641574
-82.490886	27.181983	1.646579
-82.867918	34.436692	1.651584
-82.919939	27.448457	1.656589
-83.097380	27.011021	1.661594
-83.786644	35.543101	1.666598
-84.338289	31.511115	1.671603
-84.855081	32.208440	1.676608
-84.369051	31.808642	1.681613
-84.276224	29.428347	1.686618
-84.673061	30.576128	1.691622
-84.495861	26.300568	1.696627
-84.857404	35.665381	1.701632
-85.376570	31.652197	1.706637
-86.000009	30.922368	1.711642
-86.393105	36.316859	1.716646
-86.384153	32.522121	1.721651
-86.443131	28.406148	1.726656
-86.544024	24.826774	1.731661
-86.523908	33.203830	1.736666
-87.487810	28.274852	1.741670
-87.623332	19.311272	1.746675
-88.038583	32.069165	1.751680
-87.881139	25.437080	1.756685
-87.863377	23.316023	1.761690
-88.639695	38.158554	1.766694
-89.011057	23.737273	1.771699
-89.137284	23.065753	1.776704
-89.006714	28.382475	1.781709
-89.076346	31.779540	1.786714
-89.465948	26.138177	1.791718
-90.090877	22.894905	1.796723
-90.998605	21.423426	1.801728
-91.170596	26.806133	1.806733
-90.615483	31.982155	1.811738
-91.212584	26.535496	1.816742
-90.801013	22.257705	1.821747
-90.960436	21.382328	1.826752
-91.373421	27.523161	1.831757
-91.970554	20.211860	1.836762
-92.473371	27.260155	1.841766
-92.409815	35.982620	1.846771
-92.866224	28.653682	1.851776
-92.933409	22.591747	1.856781
-93.801843	24.256082	1.861786
-94.192722	30.474652	1.866790
-94.118927	24.640095	1.871795
-94.012318	27.579580	1.876800
-93.854270	28.654004	1.881805
-94.113392	23.503188	1.886810
-94.427518	31.693387	1.891814
-95.027771	22.413677	1.896819
-95.395533	31.645247	1.901824
-95.739446	28.076638	1.906829
-95.258624	32.004443	1.911834
-95.916317	30.811671	1.916838
-96.495080	22.220661	1.921843
-96.793491	36.651744	1.926848
-97.130554	22.707706	1.931853
-96.772919	23.738292	1.936858
-97.095258	26.801054	1.941862
-97.134771	19.087036	1.946867
-97.984630	24.922425	1.951872
-98.563454	31.137725	1.956877
-98.427205	28.477083	1.961882
-98.774490	27.150734	1.966886
-98.701805	22.355873	1.971891
-98.807252	20.895835	1.976896
-99.331556	20.897712	1.981901
-99.090057	14.742245	1.986906
-100.108132	19.769247	1.991910
-100.345513	13.013994	1.996915
-100.278329	15.374207	2.006912
-100.152655	20.522214	2.016909
-99.385765	24.138265	2.026906
-99.228211	23.227637	2.036902
-98.719137	22.562363	2.046899
-97.998493	24.250074	2.056896
-97.707467	19.851306	2.066893
-96.674672	24.160060	2.076890
-96.165279	19.822450	2.086886
-96.130384	30.344659	2.096883
-95.627210	30.950817	2.106880
-95.107495	20.260705	2.116877
-94.767036	21.939239	2.126874
-93.575078	22.909210	2.136870
-93.362003	26.215696	2.146867
-93.486091	27.350127	2.156864
-92.150871	23.778780	2.166861
-91.937361	25.468466	2.176858
-91.939531	24.301380	2.186854
-90.791395	24.488604	2.196851
-90.443354	28.135158	2.206848
-90.179296	28.771056	2.216845
-89.500656	32.386285	2.226842
-88.998105	26.285747	2.236838
-88.519305	17.447110	2.246835
-87.646080	22.293620	2.256832
-87.270457	20.965316	2.266829
-87.247125	20.206668	2.276826
-86.804274	28.076685	2.286822
-86.033912	29.083343	2.296819
-85.510484	25.930745	2.306816
-84.287767	19.761121	2.316813
-84.569598	22.408009	2.326810
-84.137222	23.755702	2.336806
-83.700577	27.280240	2.346803
-82.828056	30.991002	2.356800
-82.509519	33.276261	2.366797
-82.058229	23.898335	2.376794
-80.994711	21.808596	2.386790
-80.938087	27.259073	2.396787
-80.848087	23.747527	2.406784
-80.097868	21.707690	2.416781
-79.393827	20.823898	2.426778
-78.872378	28.063307	2.436774
-78.059759	29.750736	2.446771
-78.048575	30.755832	2.456768
-77.758130	32.728552	2.466765
-76.819135	26.667010	2.476762
-76.262091	28.318000	2.486758
-75.941920	29.427164	2.496755
-75.696768	34.096699	2.506752
-74.914192	34.595587	2.516749
-74.664048	30.743650	2.526746
-73.675835	32.075248	2.536742
-73.201586	31.955909	2.546739
-73.121220	24.003976	2.556736
-72.666168	26.086203	2.566733
-71.733305	20.556174	2.576730
-71.455824	24.743998	2.586726
-70.936431	30.653433	2.596723
-69.993513	26.386715	2.606720
-69.672271	29.571559	2.616717
-69.934201	30.035336	2.626714
-69.467854	21.260196	2.636710
-68.558268	27.337622	2.646707
-67.530465	27.793464	2.656704
-66.964268	22.983437	2.666701
-66.773591	28.426677	2.676698
-66.569289	31.952525	2.686694
-66.453267	30.316258	2.696691
-65.516096	38.154820	2.706688
-64.871953	29.208147	2.716685
-63.825657	21.043338	2.726682
-63.931194	24.927792	2.736678
-63.403479	18.742494	2.746675
-63.300005	20.276316	2.756672
-62.339152	25.871177	2.766669
-61.876886	25.709270	2.776666
-61.602903	26.578970	2.786662
-60.497335	22.908674	2.796659
-60.189254	23.333613	2.806656
-60.153711	21.683286	2.816653
-59.734765	25.387765	2.826650
-58.878103	26.103086	2.836646
-58.297675	24.261558	2.846643
-57.492210	27.653580	2.856640
-57.272073	23.048914	2.866637
-57.084331	25.434024	2.876634
-56.659716	26.641549	2.886630
-55.842823	28.576706	2.896627
-55.694694	30.322837	2.906624
-54.977652	20.776431	2.916621
-54.077747	20.991696	2.926618
-53.745637	28.881897	2.936614
-53.508012	25.477379	2.946611
-52.571355	24.598807	2.956608
-52.210566	26.814656	2.966605
-52.147619	23.820742	2.976602
-51.639960	25.189877	2.986598
-50.720143	28.553569	2.996595
-50.483405	28.099256	3.006592
-49.681312	20.330266	3.016589
-49.177091	24.839388	3.026586
-49.068724	27.455573	3.036582
-48.676679	19.619910	3.046579
-48.179575	27.714433	3.056576
-47.122650	31.610362	3.066573
-46.494314	28.629394	3.076570
-46.188212	26.008886	3.086566
-46.089589	32.827046	3.096563
-45.707867	27.036197	3.106560
-44.495319	22.136689	3.116557
-44.588804	26.309170	3.126554
-43.926595	27.243274	3.136550
-43.201433	36.359675	3.146547
-43.008231	31.455512	3.156544
-42.305452	29.833404	3.166541
-41.589776	34.126374	3.176538
-41.376200	27.167484	3.186534
-41.176147	32.854153	3.196531
-39.870275	28.104578	3.206528
-39.598286	24.685244	3.216525
-39.335566	23.144506	3.226522
-39.391116	25.859149	3.236518
-38.446199	26.348845	3.246515
-38.090627	29.471022	3.256512
-37.145672	28.633507	3.266509
-36.868458	26.267982	3.276506
-36.504323	28.105990	3.286502
-35.601965	27.792528	3.296499
-35.336246	31.801682	3.306496
-35.205800	27.870797	3.316493
-33.805617	30.927123	3.326490
-33.316329	28.837904	3.336486
-33.256320	31.104647	3.346483
-33.273659	29.386455	3.356480
-32.702214	26.399283	3.366477
-31.984025	19.101757	3.376474
-31.365760	30.662792	3.386470
-30.649149	25.763602	3.396467
-30.231756	26.326847	3.406464
-29.948512	24.606987	3.416461
-28.748116	25.480452	3.426458
-28.741504	27.972990	3.436454
-28.664478	29.590950	3.446451
-27.907382	28.521135	3.456448
-27.154417	22.030522	3.466445
-26.932450	18.871493	3.476442
-26.361775	21.885075	3.486438
-25.147734	20.372334	3.496435
-25.296826	21.056459	3.506432
-25.049828	23.198311	3.516429
-24.666902	24.938484	3.526426
-23.487875	26.388256	3.536422
-23.479175	28.118708	3.546419
-22.669811	23.290574	3.556416
-21.937837	28.627275	3.566413
-21.545677	23.431580	3.576410
-21.770043	22.258194	3.586406
-21.014178	23.099527	3.596403
-20.429342	30.301109	3.606400
-19.768512	35.385285	3.616397
-19.021744	25.850954	3.626394
-18.991203	22.023852	3.636390
-18.484579	24.950278	3.646387
-17.415258	26.991450	3.656384
-17.244038	24.537747	3.666381
-16.960844	33.489724	3.676378
-16.468717	21.889219	3.686374
-15.138818	26.966097	3.696371
-15.339096	31.067574	3.706368
-15.171672	28.765186	3.716365
-14.112605	28.763163	3.726362
-13.667235	34.227095	3.736358
-13.582896	36.461815	3.746355
-12.863387	29.524267	3.756352
-12.586004	27.921443	3.766349
-11.653263	28.351122	3.776346
-10.923676	29.692329	3.786342
-10.611388	29.480928	3.796339
-10.395763	27.797926	3.806336
-10.086089	26.106000	3.816333
-9.040077	27.200220	3.826330
-8.954135	31.332581	3.836326
-8.128232	27.963656	3.846323
-7.546410	25.389992	3.856320
-6.929304	22.672798	3.866317
-7.191101	33.353992	3.876314
-6.268342	31.981897	3.886310
-6.005803	22.466891	3.896307
-5.164896	26.646858	3.906304
-4.647892	33.600209	3.916301
-4.773406	28.470206	3.926298
-3.883251	31.848934	3.936294
-3.528666	46.181516	3.946291
-2.927811	49.856093	3.956288
-2.400562	58.908072	3.966285
-2.234192	67.506877	3.976282
-1.425077	76.175693	3.986278
-1.248327	90.183529	3.996275
-0.727379	111.673069	4.006272
0.000000	121.373339	4.011277
0.123988	121.576861	4.016282
0.327699	126.671206	4.021286
0.107052	134.480897	4.026291
0.249953	130.972388	4.031296
0.423497	132.045841	4.036301
0.017068	132.557904	4.041306
0.597176	143.005479	4.046310
0.708674	156.217157	4.051315
0.997654	152.046998	4.056320
0.321851	137.914250	4.061325
0.397704	132.217029	4.066330
0.330597	133.973280	4.071334
0.405306	145.040760	4.076339
0.783834	161.575187	4.081344
0.717500	143.130753	4.086349
0.573055	152.531090	4.091354
0.813205	128.799552	4.096358
0.530757	134.783699	4.101363
0.508834	131.401378	4.106368
0.616138	144.251579	4.111373
0.881544	161.085864	4.116378
0.819859	139.435484	4.121382
0.301524	146.559795	4.126387
0.628576	152.181693	4.131392
0.794585	156.516031	4.136397
1.054936	158.944266	4.141402
1.035541	144.374912	4.146406
0.651508	126.782197	4.151411
0.588168	127.786869	4.156416
0.683323	137.138032	4.161421
0.821484	156.163832	4.166426
0.916297	158.358186	4.171430
0.673577	153.557789	4.176435
0.509613	158.313257	4.181440
0.658432	166.466193	4.186445
0.545087	171.440698	4.191450
1.036761	166.052299	4.196454
0.983251	171.511372	4.201459
1.263345	170.409943	4.206464
1.120929	169.219897	4.211469
1.019756	163.585758	4.216474
1.317922	161.966367	4.221478
0.897328	157.073426	4.226483
0.805320	147.627649	4.231488
0.683897	145.332364	4.236493
1.013923	164.357938	4.241498
1.224240	163.123414	4.246502
0.918729	157.678524	4.251507
0.997536	161.737132	4.256512
1.289333	162.252491	4.261517
1.005060	158.048221	4.266522
1.110291	137.262786	4.271526
0.784203	143.326758	4.276531
1.376342	151.379985	4.281536
1.075063	150.876093	4.286541
0.836049	150.693882	4.291546
0.900766	149.397492	4.296550
1.167914	167.910988	4.301555
1.086025	155.285776	4.306560
1.124589	168.349696	4.311565
1.044917	163.239706	4.316570
1.016263	157.261415	4.321574
1.058570	167.853623	4.326579
0.873123	164.542811	4.331584
1.303405	171.262155	4.336589
0.934707	168.011617	4.341594
1.338248	159.281265	4.346598
0.963293	173.186582	4.351603
1.200044	167.238024	4.356608
1.369876	167.700337	4.361613
1.071446	172.153753	4.366618
1.295785	158.627531	4.371622
1.388116	167.300634	4.376627
1.228736	164.629926	4.381632
1.362508	154.968169	4.386637
1.257965	169.151296	4.391642
1.345578	167.543220	4.396646
1.061044	174.447580	4.401651
1.249687	178.708337	4.406656
1.467701	179.244670	4.411661
1.278602	190.739939	4.416666
2.000888	183.576117	4.421670
1.536304	186.008335	4.426675
1.168601	168.935545	4.431680
1.448938	166.027516	4.436685
1.546331	183.341823	4.441690
1.284436	167.298176	4.446694
1.848907	186.093249	4.451699
1.409769	175.076724	4.456704
1.654562	171.815860	4.461709
1.334038	176.323835	4.466714
1.552408	176.161240	4.471718
1.633086	192.096269	4.476723
1.648413	184.402989	4.481728
1.661857	185.797880	4.486733
1.641394	186.597865	4.491738
1.920070	180.611692	4.496742
1.505055	179.415689	4.501747
1.296786	177.583433	4.506752
1.571627	176.446172	4.511757
1.667482	193.053589	4.516762
1.910973	196.882256	4.521766
1.977804	190.624568	4.526771
1.324140	185.957775	4.531776
1.422964	172.481287	4.536781
1.527577	184.292641	4.541786
1.650347	181.865544	4.546790
1.397333	194.099547	4.551795
1.789827	189.476811	4.556800
2.192449	188.378317	4.561805
2.051173	196.492984	4.566810
2.118272	179.436131	4.571814
2.065583	191.326069	4.576819
2.063175	189.236042	4.581824
1.902303	176.832420	4.586829
1.629903	168.868042	4.591834
1.792894	173.460274	4.596838
1.753959	182.260342	4.601843
2.148698	188.467730	4.606848
2.048174	180.411607	4.611853
1.795186	180.772431	4.616858
1.748438	170.868702	4.621862
1.904321	185.111309	4.626867
1.752241	186.570747	4.631872
2.105467	190.275521	4.636877
1.717066	196.727756	4.641882
1.884570	186.006083	4.646886
1.803788	195.207989	4.651891
1.898846	185.998036	4.656896
2.159404	189.394437	4.661901
1.722306	188.077976	4.666906
2.067681	198.562013	4.671910
2.070303	197.645244	4.676915
2.016390	190.762900	4.681920
2.209296	187.766320	4.686925
1.898983	188.314689	4.691930
2.195079	186.635754	4.696934
2.173674	192.061413	4.701939
2.012164	193.736984	4.706944
2.218383	183.202377	4.711949
2.094595	186.406679	4.716954
2.190571	198.033902	4.721958
1.905726	194.053959	4.726963
2.106491	195.300595	4.731968
2.011575	196.655189	4.736973
2.075979	189.918440	4.741978
2.267764	194.696125	4.746982
2.228979	196.713774	4.751987
2.529018	199.454703	4.756992
2.156873	197.265167	4.761997
2.264136	198.026189	4.767002
2.349792	196.186200	4.772006
1.896602	202.620436	4.777011
2.502322	211.049693	4.782016
2.705402	209.749769	4.787021
2.198171	216.990663	4.792026
2.446368	208.574717	4.797030
2.466944	214.515132	4.802035
2.426043	210.462710	4.807040
2.335723	200.377141	4.812045
2.039123	206.212811	4.817050
2.543166	213.590541	4.822054
2.720007	219.585340	4.827059
2.885890	210.361991	4.832064
2.753756	196.789972	4.837069
2.046918	204.245667	4.842074
2.458951	195.285900	4.847078
2.231764	201.966913	4.852083
2.117475	203.251506	4.857088
2.503084	216.738763	4.862093
2.316406	227.763668	4.867098
2.570190	227.512253	4.872102
2.572280	229.000379	4.877107
2.941634	229.059174	4.882112
3.218571	224.271928	4.887117
2.422509	212.923488	4.892122
2.775245	207.300052	4.897126
2.264813	208.197681	4.902131
2.446561	215.232870	4.907136
2.786093	226.255954	4.912141
2.773081	222.963397	4.917146
2.574470	222.964518	4.922150
2.203362	231.516638	4.927155
2.294233	229.131209	4.932160
2.560663	222.991070	4.937165
2.448639	240.353268	4.942170
2.491250	223.459543	4.947174
2.714372	231.288782	4.952179
2.658641	221.403869	4.957184
3.066253	227.139549	4.962189
2.561497	223.753536	4.967194
2.978790	225.853766	4.972198
2.768631	223.364972	4.977203
3.107534	225.108792	4.982208
2.871118	227.381966	4.987213
2.928961	225.948194	4.992218
3.122956	219.384268	4.997222
3.188590	217.180195	5.002227
2.923169	233.019349	5.007232
3.098718	219.864679	5.012237
2.762047	225.008699	5.017242
3.260257	212.283827	5.022246
3.015603	232.476634	5.027251
3.075938	230.145677	5.032256
3.267120	220.648320	5.037261
3.040948	226.430530	5.042266
2.567723	220.683431	5.047270
2.641535	232.472387	5.052275
2.659421	239.290101	5.057280
2.721873	225.435415	5.062285
2.735933	225.897624	5.067290
2.488337	224.323431	5.072294
2.885642	243.117195	5.077299
2.927760	256.233482	5.082304
3.172770	253.127060	5.087309
2.759697	262.417165	5.092314
3.335982	257.723292	5.097318
3.409772	257.552329	5.102323
3.400392	250.994474	5.107328
3.727917	256.388440	5.112333
3.190147	244.015873	5.117338
3.013432	233.708182	5.122342
3.085084	238.374621	5.127347
3.444535	246.565007	5.132352
3.463096	226.455058	5.137357
2.840935	234.333716	5.142362
3.220427	235.503071	5.147366
3.043954	243.856899	5.152371
3.235717	244.992659	5.157376
3.624654	252.960148	5.162381
3.573948	255.929329	5.167386
3.120841	234.569714	5.172390
3.171676	245.512270	5.177395
3.321539	242.173160	5.182400
3.637279	252.310230	5.187405
3.155095	246.543391	5.192410
3.396572	254.067428	5.197414
3.525059	253.053989	5.202419
3.342051	259.156711	5.207424
3.583007	253.717964	5.212429
3.267669	259.798752	5.217434
3.586125	246.949950	5.222438
3.373516	241.615758	5.227443
3.495915	259.261347	5.232448
3.444152	245.441696	5.237453
3.420222	260.129919	5.242458
3.616328	247.331129	5.247462
3.356409	241.399902	5.252467
3.663589	250.754276	5.257472
3.813578	247.864419	5.262477
2.931863	248.281198	5.267482
3.485147	242.299836	5.272486
3.370559	256.509664	5.277491
3.387130	262.761720	5.282496
3.623953	252.071165	5.287501
3.457688	262.068288	5.292506
3.423301	245.108537	5.297510
3.514367	260.177407	5.302515
3.599803	248.277796	5.307520
3.665466	250.026325	5.312525
3.599975	251.251657	5.317530
3.796348	258.995653	5.322534
3.633261	260.019480	5.327539
3.503299	253.868278	5.332544
3.666040	251.325848	5.337549
3.690833	256.632908	5.342554
3.627297	252.176376	5.347558
3.328130	255.502904	5.352563
3.712564	274.130824	5.357568
3.958488	273.478983	5.362573
3.517356	271.393079	5.367578
3.617805	272.885179	5.372582
3.895172	283.115920	5.377587
4.051125	278.547046	5.382592
4.328112	276.883197	5.387597
3.759149	266.835543	5.392602
3.559913	253.072912	5.397606
3.608057	270.971996	5.402611
3.614282	290.979582	5.407616
4.019882	281.698029	5.412621
3.878720	286.919169	5.417626
3.915786	297.618387	5.422630
3.449218	293.453774	5.427635
3.502840	291.220008	5.432640
3.700935	286.761073	5.437645
3.831067	291.729516	5.442650
4.008895	281.040601	5.447654
4.105014	285.735666	5.452659
4.033711	291.128171	5.457664
4.358740	291.349180	5.462669
4.116441	297.418307	5.467674
4.412926	290.038405	5.472678
4.428044	290.816336	5.477683
3.861060	295.680179	5.482688
4.481644	290.393259	5.487693
3.872801	293.917276	5.492698
4.175822	285.748929	5.497702
4.158192	297.447387	5.502707
4.254059	287.813120	5.507712
4.115602	291.014837	5.512717
4.152552	292.933955	5.517722
4.309245	291.560102	5.522726
4.646260	287.374175	5.527731
4.018976	292.455355	5.532736
4.548743	290.288321	5.537741
4.190235	288.538099	5.542746
4.565322	281.355150	5.547750
4.459136	293.386797	5.552755
4.501044	280.598269	5.557760
4.449703	267.577932	5.562765
4.063357	269.309707	5.567770
4.439282	269.492314	5.572774
4.340963	269.924755	5.577779
4.236107	270.827283	5.582784
4.500477	275.487734	5.587789
4.116528	259.996008	5.592794
4.549785	274.053066	5.597798
4.378812	275.510307	5.602803
4.159891	282.456358	5.607808
4.003852	277.918226	5.612813
4.191710	284.812741	5.617818
4.240125	286.469711	5.622822
4.132986	278.998964	5.627827
4.147877	289.076070	5.632832
4.057100	283.038346	5.637837
4.140940	284.431577	5.642842
4.290628	295.909315	5.647846
4.040715	299.443373	5.652851
4.658449	301.512265	5.657856
4.391367	296.359111	5.662861
4.773493	307.933704	5.667866
4.635209	298.721006	5.672870
4.742858	307.054750	5.677875
4.784828	306.324934	5.682880
4.880337	300.910996	5.687885
4.238560	305.882108	5.692890
4.740872	294.783809	5.697894
4.635598	303.515986	5.702899
4.429491	307.356827	5.707904
4.755237	298.497978	5.712909
4.422323	308.498007	5.717914
4.527290	311.461500	5.722918
4.570833	304.990276	5.727923
4.480935	309.613191	5.732928
4.551239	305.770064	5.737933
4.398002	311.058912	5.742938
4.542798	309.160796	5.747942
4.498897	308.214712	5.752947
4.644019	312.061144	5.757952
4.532599	310.596734	5.762957
4.787832	318.547286	5.767962
4.914478	327.200899	5.772966
5.037310	328.841729	5.777971
4.817221	319.966028	5.782976
4.670513	316.959250	5.787981
4.898925	333.088829	5.792986
5.066732	323.991274	5.797990
5.311631	320.097784	5.802995
4.846023	314.953161	5.808000
4.858396	313.493846	5.813005
4.783966	314.670345	5.818010
4.558913	304.841970	5.823014
4.742052	322.883758	5.828019
4.609025	332.250354	5.833024
4.918477	334.806845	5.838029
5.130643	344.369060	5.843034
5.436204	344.986923	5.848038
5.147545	340.702825	5.853043
5.315138	344.402699	5.858048
5.048947	318.709709	5.863053
4.757605	315.611900	5.868058
5.080274	336.042375	5.873062
5.111429	339.545581	5.878067
4.898694	348.471050	5.883072
5.141580	336.594088	5.888077
4.973471	345.064580	5.893082
5.392959	339.210360	5.898086
5.067478	345.943491	5.903091
5.061557	338.141375	5.908096
5.293004	340.237803	5.913101
5.021268	340.695451	5.918106
5.060409	339.135619	5.923110
5.228599	344.329631	5.928115
5.312740	341.748281	5.933120
5.246595	338.685665	5.938125
5.213801	337.220887	5.943130
5.357155	343.107520	5.948134
5.542321	348.165147	5.953139
4.976736	345.627732	5.958144
5.138130	336.173505	5.963149
5.177763	349.217869	5.968154
5.109027	347.363717	5.973158
5.196685	344.569972	5.978163
4.998624	341.336679	5.983168
5.348908	342.633695	5.988173
5.126686	345.303700	5.993178
5.567452	346.867821	5.998182
5.216384	337.520182	6.003187
5.170422	346.571598	6.008192
5.656740	346.278497	6.013197
5.210379	349.550938	6.018202
5.249601	348.187713	6.023206
5.044618	345.047706	6.028211
5.295714	348.873576	6.033216
5.602904	356.459513	6.038221
5.406552	356.071952	6.043226
5.444733	343.974084	6.048230
5.641971	338.736390	6.053235
5.184449	349.483537	6.058240
5.214628	337.676452	6.063245
5.265294	350.955965	6.068250
5.083591	355.397444	6.073254
5.537078	368.708665	6.078259
5.772261	371.862465	6.083264
5.698485	365.968698	6.088269
5.180613	363.256667	6.093274
5.659268	365.938512	6.098278
5.253120	359.132454	6.103283
5.361850	351.597190	6.108288
5.525778	348.856743	6.113293
5.407755	348.120907	6.118298
5.145948	346.487291	6.123302
5.772324	357.055916	6.128307
5.682181	358.052207	6.133312
5.681309	347.077670	6.138317
5.495172	342.567085	6.143322
5.889637	342.326653	6.148326
5.687271	352.489820	6.153331
5.617917	351.091756	6.158336
5.660517	342.051976	6.163341
5.479694	350.757499	6.168346
5.710488	357.041179	6.173350
5.790017	341.940900	6.178355
5.206711	334.110685	6.183360
5.491403	333.727289	6.188365
5.578304	347.112784	6.193370
5.519239	329.485174	6.198374
5.231166	314.879556	6.203379
4.803049	325.689505	6.208384
5.181563	332.504391	6.213389
5.512126	342.253821	6.218394
5.392242	342.418525	6.223398
5.587312	353.258793	6.228403
5.419799	347.074001	6.233408
5.423929	347.550384	6.238413
5.360210	344.490227	6.243418
5.488426	341.490792	6.248422
5.811412	334.737392	6.253427
5.247188	341.170402	6.258432
5.365791	334.825964	6.263437
5.629771	334.804209	6.268442
5.605294	332.890063	6.273446
5.407944	319.304048	6.278451
5.386172	319.048841	6.283456
5.445382	298.115509	6.288461
5.218201	308.460526	6.293466
4.802992	319.701040	6.298470
5.486287	335.653342	6.303475
5.228393	342.642461	6.308480
5.657237	322.932310	6.313485
5.870400	337.541667	6.318490
5.720814	338.254970	6.323494
5.514441	316.272104	6.328499
5.244897	312.289010	6.333504
5.509430	300.553324	6.338509
5.366838	312.738788	6.343514
5.449193	308.865354	6.348518
5.033065	307.586851	6.353523
4.975682	327.068311	6.358528
5.440460	326.629209	6.363533
5.452267	340.098732	6.368538
5.510075	331.683302	6.373542
5.590879	329.042129	6.378547
5.752442	336.121947	6.383552
5.898579	325.479081	6.388557
5.474716	312.251234	6.393562
5.094478	312.081902	6.398566
4.818659	311.370073	6.403571
5.240040	324.712803	6.408576
5.173883	331.903454	6.413581
5.196815	344.507808	6.418586
5.296593	342.701477	6.423590
5.581640	335.702972	6.428595
5.484106	328.710177	6.433600
5.892125	333.356871	6.438605
5.283862	341.594070	6.443610
5.293206	346.802000	6.448614
5.567230	342.914543	6.453619
5.321860	351.395439	6.458624
5.519053	339.189511	6.463629
5.493595	344.360277	6.468634
5.178655	348.074681	6.473638
5.372555	341.017540	6.478643
5.387063	339.521564	6.483648
5.554378	334.048985	6.488653
5.410251	335.287417	6.493658
5.114080	341.265525	6.498662
5.285994	340.497463	6.503667
5.096745	345.659484	6.508672
5.429527	338.454101	6.513677
5.343498	345.689378	6.518682
5.282830	342.644404	6.523686
5.402774	342.743726	6.528691
4.924408	354.051922	6.533696
5.139543	338.486766	6.538701
5.045804	340.935761	6.543706
5.236384	346.425295	6.548710
5.699465	345.838983	6.553715
5.127412	339.030063	6.558720
5.523592	347.222819	6.563725
5.638234	345.760708	6.568730
5.560994	347.035935	6.573734
5.605548	341.591533	6.578739
5.164939	338.067826	6.583744
5.569170	331.983401	6.588749
5.455479	340.515042	6.593754
5.235758	341.315012	6.598758
5.717381	336.941999	6.603763
5.457102	339.867398	6.608768
5.703757	338.271399	6.613773
5.494767	344.880308	6.618778
5.462452	351.165242	6.623782
5.776911	336.542606	6.628787
5.636781	348.513905	6.633792
5.921602	340.100615	6.638797
5.534665	341.764226	6.643802
5.359878	350.439943	6.648806
5.585248	343.674751	6.653811
5.601972	349.374346	6.658816
5.578061	321.019247	6.663821
5.049134	332.978819	6.668826
5.257137	332.537657	6.673830
5.574045	341.069566	6.678835
5.497311	339.818733	6.683840
5.651448	335.123764	6.688845
5.379543	324.963151	6.693850
5.191085	315.014577	6.698854
5.523592	315.101463	6.703859
5.266967	318.249412	6.708864
5.440901	322.415563	6.713869
5.587646	337.075654	6.718874
5.583584	320.540551	6.723878
5.538359	308.007612	6.728883
5.146847	311.488517	6.733888
5.142418	307.662277	6.738893
5.334890	323.717085	6.743898
5.786925	330.114544	6.748902
5.480829	314.670669	6.753907
5.289251	310.889365	6.758912
5.375893	303.718952	6.763917
4.990094	318.532439	6.768922
5.505555	328.608339	6.773926
5.905030	325.254598	6.778931
5.246632	329.499697	6.783936
5.369236	304.459805	6.788941
5.347773	324.685106	6.793946
5.170523	332.135722	6.798950
5.300026	334.701134	6.803955
5.597427	346.563427	6.808960
5.637691	336.425803	6.813965
5.654002	344.350344	6.818970
5.360627	324.664930	6.823974
5.618006	313.055315	6.828979
5.394629	321.795181	6.833984
5.395618	320.634501	6.838989
5.558685	321.596739	6.843994
5.459110	322.493563	6.848998
5.692949	313.928989	6.854003
5.230034	317.177621	6.859008
5.539963	304.621904	6.864013
5.157009	313.045112	6.869018
5.438586	316.741335	6.874022
5.445536	311.025147	6.879027
5.055726	325.839600	6.884032
5.587565	313.019705	6.889037
5.395366	315.455567	6.894042
5.322551	318.342485	6.899046
5.535991	309.503866	6.904051
5.158444	321.086904	6.909056
5.352879	305.705051	6.914061
5.530823	315.148301	6.919066
5.362961	311.732344	6.924070
5.350071	319.446826	6.929075
5.079124	324.146231	6.934080
5.606799	331.389295	6.939085
5.852097	329.768660	6.944090
5.379632	318.223911	6.949094
5.632238	320.563478	6.954099
5.322056	319.946413	6.959104
5.647514	312.803912	6.964109
5.362879	304.822346	6.969114
5.174099	312.311163	6.974118
5.128227	313.551903	6.979123
5.169194	322.818215	6.984128
5.398506	333.265192	6.989133
5.677861	336.809957	6.994138
5.310289	329.922065	6.999142
5.740310	321.541320	7.004147
5.479635	324.588226	7.009152
5.489095	317.147716	7.014157
5.273950	312.456165	7.019162
5.454706	319.078002	7.024166
5.874905	312.945269	7.029171
5.550153	314.575120	7.034176
5.253172	320.662171	7.039181
5.158215	315.360897	7.044186
5.303122	320.972904	7.049190
5.500388	306.257985	7.054195
5.126945	314.981310	7.059200
5.467387	312.000971	7.064205
5.533171	316.285720	7.069210
5.123709	318.179761	7.074214
5.245840	318.002387	7.079219
5.275965	325.785926	7.084224
5.440447	334.198786	7.089229
5.377458	343.944787	7.094234
5.223597	339.622332	7.099238
5.885581	348.368424	7.104243
5.169005	330.906887	7.109248
5.418973	329.086689	7.114253
5.640477	337.613053	7.119258
5.535044	338.269732	7.124262
5.561020	317.798838	7.129267
5.377918	318.604890	7.134272
5.298908	314.886965	7.139277
5.152973	314.866161	7.144282
5.195952	319.803832	7.149286
5.564845	331.282171	7.154291
5.376550	340.915297	7.159296
5.480938	335.320228	7.164301
5.386553	331.072100	7.169306
5.592977	341.658024	7.174310
5.521489	316.789488	7.179315
4.991340	315.570868	7.184320
5.184204	329.752054	7.189325
5.271631	354.813546	7.194330
5.264508	352.671002	7.199334
5.277760	339.325416	7.204339
5.462651	350.556856	7.209344
5.458299	346.455049	7.214349
5.442595	346.759695	7.219354
5.262612	350.196476	7.224358
5.554326	346.209412	7.229363
5.588604	347.538920	7.234368
5.421610	341.529553	7.239373
5.565341	350.360895	7.244378
5.492786	344.857118	7.249382
5.715609	351.066543	7.254387
5.520243	333.673956	7.259392
5.418586	324.452921	7.264397
5.315001	323.909052	7.269402
5.064432	330.034410	7.274406
5.707241	337.609665	7.279411
5.465428	338.782158	7.284416
5.193174	335.866860	7.289421
5.541415	332.583047	7.294426
5.244324	346.032096	7.299430
5.549252	347.928345	7.304435
5.784616	346.168864	7.309440
5.346255	323.728679	7.314445
5.600575	314.514034	7.319450
5.401522	318.540072	7.324454
5.321989	313.855312	7.329459
5.386384	320.085084	7.334464
5.352395	310.196718	7.339469
5.002578	320.703185	7.344474
5.225298	330.744297	7.349478
5.614228	330.892199	7.354483
5.432561	342.156487	7.359488
5.732866	336.985618	7.364493
5.522899	325.565692	7.369498
5.572415	322.038635	7.374502
5.080548	317.344866	7.379507
5.317908	314.958104	7.384512
5.616033	315.489589	7.389517
5.356189	325.913315	7.394522
5.413064	319.870316	7.399526
5.401299	308.290481	7.404531
4.938529	320.436028	7.409536
5.858710	327.666810	7.414541
5.731053	326.176768	7.419546
5.191197	317.758498	7.424550
5.484166	312.028587	7.429555
5.368670	313.541184	7.434560
5.301250	306.494885	7.439565
5.370726	317.817589	7.444570
5.322142	321.089501	7.449574
5.290769	321.629464	7.454579
5.564064	332.756505	7.459584
5.460460	331.922394	7.464589
5.317116	330.215534	7.469594
5.207645	328.036239	7.474598
5.572301	336.179051	7.479603
5.846242	338.013136	7.484608
5.583604	316.690595	7.489613
5.888527	316.995430	7.494618
5.648027	319.857574	7.499622
5.573490	317.836966	7.504627
5.278406	315.293035	7.509632
4.962024	312.877520	7.514637
5.356982	312.047048	7.519642
4.938808	318.667233	7.524646
5.120325	318.858192	7.529651
4.970207	322.137708	7.534656
5.576166	327.979358	7.539661
5.708889	342.295885	7.544666
5.612040	346.738138	7.549670
5.559219	316.930779	7.554675
5.394277	322.043197	7.559680
5.501765	315.749142	7.564685
5.176074	320.722877	7.569690
5.293290	311.202862	7.574694
5.734492	316.582108	7.579699
5.493332	322.521324	7.584704
5.403035	309.680233	7.589709
5.448999	315.051986	7.594714
5.660723	324.484727	7.599718
5.683088	306.927050	7.604723
5.016866	319.191750	7.609728
5.376591	312.897350	7.614733
5.416388	314.821723	7.619738
5.535188	314.574065	7.624742
5.599071	314.064576	7.629747
5.541665	311.832777	7.634752
5.425684	307.524296	7.639757
5.282738	313.368749	7.644762
5.254418	315.039785	7.649766
5.663702	315.690820	7.654771
5.126960	319.984378	7.659776
5.546598	318.378243	7.664781
5.339137	314.995170	7.669786
5.377002	320.804813	7.674790
5.458317	313.072052	7.679795
5.634927	313.183221	7.684800
5.784881	308.589383	7.689805
5.705028	308.866647	7.694810
5.615059	312.636699	7.699814
5.370373	311.767500	7.704819
5.466044	315.862331	7.709824
5.554411	316.152639	7.714829
5.231801	316.458971	7.719834
5.555854	311.764046	7.724838
5.435055	320.192276	7.729843
5.424553	313.895326	7.734848
5.536771	311.948727	7.739853
5.464960	310.434068	7.744858
5.889284	317.560231	7.749862
5.161704	299.982753	7.754867
5.314122	313.562003	7.759872
5.474443	319.004734	7.764877
5.419414	318.448697	7.769882
5.620362	311.107067	7.774886
5.888907	311.042234	7.779891
5.187417	304.625664	7.784896
5.378668	295.985662	7.789901
5.286000	301.288077	7.794906
5.421725	299.064123	7.799910
5.364720	288.069407	7.804915
5.207721	300.815927	7.809920
5.342237	304.740567	7.814925
5.518325	309.960195	7.819930
5.529912	314.969348	7.824934
5.584426	301.469486	7.829939
5.452604	301.334376	7.834944
5.519068	296.113868	7.839949
5.297741	295.350120	7.844954
4.908116	291.496481	7.849958
5.536522	300.903264	7.854963
5.315888	311.243944	7.859968
5.331873	308.149807	7.864973
5.620661	306.996223	7.869978
5.471312	316.946093	7.874982
5.710175	311.164451	7.879987
5.058508	311.930634	7.884992
5.321869	297.332265	7.889997
5.003508	317.904855	7.895002
5.338522	314.991118	7.900006
5.549568	312.977577	7.905011
5.685166	309.026779	7.910016
5.521258	306.814949	7.915021
5.538639	315.838417	7.920026
5.516632	311.461822	7.925030
5.516688	306.917123	7.930035
5.257702	295.413472	7.935040
5.407759	302.015612	7.940045
5.437115	294.014522	7.945050
5.467023	306.602401	7.950054
5.709071	297.113559	7.955059
5.504623	311.552764	7.960064
5.674878	291.230414	7.965069
5.590280	301.256193	7.970074
5.292207	297.804340	7.975078
5.424305	287.163426	7.980083
5.441405	289.255708	7.985088
5.327498	293.638514	7.990093
5.339432	297.481597	7.995098
5.224340	301.899919	8.000102
5.357258	299.131161	8.005107
5.280062	293.145153	8.010112
5.306740	288.329851	8.015130
5.471562	298.932431	8.020147
5.714697	297.742473	8.025165
5.666599	293.292216	8.030182
5.247645	294.729524	8.035200
5.240249	291.770835	8.040218
5.360816	297.971068	8.045235
5.429663	303.103905	8.050253
5.417014	298.374128	8.055270
4.978082	295.949740	8.060288
5.301680	301.243288	8.065306
5.520325	308.290219	8.070323
5.298337	312.749035	8.075341
5.557489	310.736530	8.080358
5.779205	315.843026	8.085376
5.707106	323.513378	8.090394
5.485154	303.991405	8.095411
5.331105	319.075645	8.100429
5.858952	312.845927	8.105446
5.286271	309.070810	8.110464
5.577425	314.556494	8.115482
5.504911	308.339985	8.120499
5.454515	313.431816	8.125517
5.725589	316.325914	8.130534
5.630036	314.872211	8.135552
5.296518	302.020179	8.140570
5.523061	301.725779	8.145587
5.548094	316.621796	8.150605
5.675641	312.884373	8.155622
5.771387	318.093461	8.160640
5.260883	302.891472	8.165658
5.479866	308.629283	8.170675
5.415867	320.136234	8.175693
5.577172	311.344827	8.180710
5.913469	322.599252	8.185728
5.365576	312.687419	8.190746
5.852298	323.950149	8.195763
5.337671	311.964273	8.200781
5.668850	307.205916	8.205798
5.652189	318.604770	8.210816
5.398250	324.420642	8.215834
5.773639	310.736057	8.220851
5.659032	316.301883	8.225869
5.709248	314.413551	8.230886
5.369665	325.266003	8.235904
5.463750	321.506949	8.240922
5.868532	314.328093	8.245939
5.482174	311.037328	8.250957
5.544406	311.360503	8.255974
5.570214	314.713839	8.260992
5.775987	319.891166	8.266010
5.830982	313.155366	8.271027
5.420127	315.560712	8.276045
5.598845	312.445109	8.281062
5.660253	315.770323	8.286080
5.685531	320.884388	8.291098
5.575683	315.731000	8.296115
5.336068	328.075956	8.301133
5.417835	317.300781	8.306150
5.534458	319.906200	8.311168
5.479530	324.368508	8.316186
6.033668	315.467702	8.321203
5.392558	326.850293	8.326221
5.570297	319.477018	8.331238
5.515198	337.117001	8.336256
5.747569	347.930549	8.341274
5.917157	351.950142	8.346291
5.714598	339.729543	8.351309
6.064367	337.431449	8.356326
5.741788	329.854887	8.361344
5.372026	327.418079	8.366362
5.878094	343.181568	8.371379
6.012586	358.747184	8.376397
5.755908	345.586221	8.381414
5.465434	339.129991	8.386432
5.995315	341.781565	8.391450
6.174546	340.123134	8.396467
5.549797	331.022734	8.401485
5.579722	333.402082	8.406502
5.959727	343.029671	8.411520
6.011340	353.220775	8.416538
6.054022	332.443780	8.421555
5.688483	330.305815	8.426573
5.947129	319.810495	8.431590
5.908467	314.619661	8.436608
5.433764	325.881170	8.441626
5.908865	331.781935	8.446643
6.092677	345.672329	8.451661
5.932932	332.859649	8.456678
6.273097	328.524905	8.461696
5.866254	324.052544	8.466714
6.050630	316.192157	8.471731
5.835671	323.398526	8.476749
5.555088	326.199873	8.481766
5.426188	320.564994	8.486784
5.896255	338.719341	8.491802
6.306098	349.073636	8.496819
5.838508	352.905282	8.501837
5.983878	348.001475	8.506854
5.887374	348.627398	8.511872
5.505962	354.111273	8.516890
6.061269	345.672460	8.521907
6.334905	347.875247	8.526925
6.315748	345.669804	8.531942
5.947050	334.282299	8.536960
5.512329	330.580420	8.541978
5.872887	327.244844	8.546995
5.785150	346.328402	8.552013
5.975211	350.110508	8.557030
6.015769	344.514039	8.562048
6.011543	347.757115	8.567066
6.201719	349.133620	8.572083
5.946154	348.480795	8.577101
6.116159	361.757378	8.582119
6.388965	346.557662	8.587136
5.910534	339.220091	8.592154
6.090861	337.017405	8.597171
5.897250	330.538579	8.602189
5.953902	338.038677	8.607207
6.206087	342.597745	8.612224
6.162127	349.102589	8.617242
5.984985	337.767363	8.622259
6.233443	344.145355	8.627277
6.372191	341.939108	8.632295
6.322961	321.019576	8.637312
6.085568	319.150431	8.642330
5.913726	318.127650	8.647347
5.792615	327.167813	8.652365
5.737330	323.238307	8.657383
5.913055	331.517075	8.662400
6.087101	346.326599	8.667418
6.100162	346.823416	8.672435
6.194505	355.912619	8.677453
6.316381	360.767676	8.682471
6.383396	346.665714	8.687488
6.112184	352.814006	8.692506
6.172791	331.993015	8.697523
5.807620	340.940181	8.702541
5.886661	344.983592	8.707559
6.175282	347.768224	8.712576
6.072443	360.862188	8.717594
6.055133	350.434985	8.722611
5.944278	356.216694	8.727629
5.987723	357.251385	8.732647
6.314482	350.739104	8.737664
5.954984	352.208217	8.742682
6.131796	351.980978	8.747699
6.176775	359.783049	8.752717
6.147322	358.024486	8.757735
6.305762	354.691604	8.762752
5.920337	358.599516	8.767770
6.152994	353.029750	8.772787
6.460938	360.511949	8.777805
6.291415	359.004830	8.782823
6.708545	356.246387	8.787840
6.394927	357.581371	8.792858
6.360686	355.581230	8.797875
6.293435	357.181734	8.802893
6.113007	361.192847	8.807911
6.411817	350.295284	8.812928
6.078670	361.761527	8.817946
6.183276	347.963719	8.822963
6.330721	356.185867	8.827981
6.029841	356.084606	8.832999
6.390610	359.608731	8.838016
5.971851	362.345142	8.843034
6.152886	359.707193	8.848051
6.477804	346.894215	8.853069
6.062691	353.675113	8.858087
6.322900	351.818496	8.863104
5.764252	365.060213	8.868122
6.204227	363.413896	8.873139
6.824478	379.871392	8.878157
6.319895	371.006763	8.883175
6.425603	359.047443	8.888192
5.996428	358.425375	8.893210
6.212204	370.617763	8.898227
6.412730	372.581212	8.903245
6.550718	380.458456	8.908263
6.615924	384.569602	8.913280
6.416268	373.053268	8.918298
6.174824	368.550707	8.923315
6.575208	382.232152	8.928333
6.320239	384.344286	8.933351
6.708836	382.550388	8.938368
6.031694	371.646116	8.943386
6.500667	374.552098	8.948403
6.535139	386.311961	8.953421
6.194551	380.341944	8.958439
6.514069	381.770782	8.963456
6.492303	383.996608	8.968474
6.620225	384.476512	8.973491
6.782661	377.959688	8.978509
6.143013	375.162933	8.983527
6.825959	377.811753	8.988544
6.495993	383.341948	8.993562
6.021641	383.062804	8.998579
6.453904	380.979861	9.003597
6.306806	392.549800	9.008615
6.854159	382.607288	9.013632
6.434115	393.829210	9.018650
6.501022	385.791687	9.023667
6.460677	386.181115	9.028685
6.359991	383.732994	9.033703
6.408483	381.585447	9.038720
6.549052	381.406117	9.043738
6.120100	378.052214	9.048755
6.815891	377.828562	9.053773
6.603957	380.289216	9.058791
6.611664	385.230948	9.063808
6.058455	380.501322	9.068826
6.496430	379.972417	9.073843
6.390153	383.442261	9.078861
6.396461	391.140920	9.083879
6.407051	372.413620	9.088896
6.329366	381.530282	9.093914
6.220686	392.946759	9.098931
6.654234	404.390838	9.103949
6.982163	401.530224	9.108967
6.962178	403.768945	9.113984
6.314777	391.981387	9.119002
6.477343	406.481516	9.124019
6.736456	395.919349	9.129037
6.743727	404.231209	9.134055
7.104475	399.176661	9.139072
6.911039	389.400746	9.144090
6.745376	383.481824	9.149107
6.895009	379.617139	9.154125
6.405579	386.071723	9.159143
6.464814	375.783297	9.164160
6.614382	383.340685	9.169178
6.559695	382.972017	9.174195
6.884020	388.123772	9.179213
6.586279	394.909597	9.184231
6.934706	405.491159	9.189248
6.697335	394.496877	9.194266
6.510906	396.116883	9.199283
7.072019	404.244324	9.204301
6.987252	398.091503	9.209319
6.826008	381.488697	9.214336
6.664535	388.838686	9.219354
6.733644	391.820591	9.224371
6.729515	383.272971	9.229389
6.551333	394.249358	9.234407
6.933121	401.815712	9.239424
6.839116	403.118934	9.244442
6.728941	406.434834	9.249459
7.054516	395.976128	9.254477
6.658476	404.321967	9.259495
6.830448	398.189992	9.264512
6.723499	407.463245	9.269530
6.632915	410.124866	9.274547
6.978537	408.368572	9.279565
6.993812	416.358220	9.284583
7.140785	424.338998	9.289600
6.869016	397.354869	9.294618
6.951851	398.202384	9.299635
7.210616	382.743984	9.304653
6.690709	382.262472	9.309671
6.830385	382.159455	9.314688
6.866036	380.010487	9.319706
7.083049	377.569991	9.324723
7.035004	374.792867	9.329741
6.799548	383.225814	9.334759
7.097079	379.689762	9.339776
6.940152	375.367482	9.344794
6.921359	389.836162	9.349811
7.120100	365.157389	9.354829
6.952421	380.633425	9.359847
7.177353	369.066413	9.364864
7.107819	380.027394	9.369882
7.018870	386.271635	9.374899
7.080347	373.860656	9.379917
7.040432	374.077609	9.384935
6.957793	375.227900	9.389952
6.887178	384.157510	9.394970
6.970628	382.797028	9.399987
7.225791	371.839552	9.405005
6.884270	376.373148	9.410023
7.205204	378.050812	9.415040
7.206894	379.028442	9.420058
7.096945	383.755218	9.425075
7.011683	385.849049	9.430093
7.010572	379.109207	9.435111
7.168291	386.599417	9.440128
7.025477	391.835259	9.445146
6.604644	393.724267	9.450163
7.251543	380.334443	9.455181
6.874640	391.424556	9.460199
7.017990	385.754404	9.465216
7.296144	383.984563	9.470234
6.856143	380.144794	9.475251
7.252851	379.620249	9.480269
6.870403	390.499118	9.485287
6.948825	374.585101	9.490304
7.112369	384.732538	9.495322
6.871483	378.585942	9.500339
7.133563	391.759263	9.505357
7.000299	410.278400	9.510375
7.363267	416.215836	9.515392
7.670152	408.078223	9.520410
7.230162	406.772062	9.525427
7.207854	384.299013	9.530445
7.167953	383.536842	9.535463
6.874168	384.807737	9.540480
6.935944	385.820802	9.545498
7.195175	410.488318	9.550515
7.195241	402.603633	9.555533
7.324373	411.459117	9.560551
7.305565	411.116302	9.565568
7.142709	407.003020	9.570586
7.357072	413.364140	9.575603
7.236230	410.032034	9.580621
7.236547	418.674312	9.585639
7.536781	417.104220	9.590656
7.294180	398.241995	9.595674
7.077858	403.364327	9.600691
7.489978	388.898570	9.605709
6.919122	396.548154	9.610727
7.432565	404.970322	9.615744
7.716560	403.124332	9.620762
6.822351	404.497502	9.625779
7.460927	408.025423	9.630797
6.987760	413.444184	9.635815
7.167187	418.826250	9.640832
7.727675	414.028293	9.645850
7.548839	420.409423	9.650867
7.473255	407.679702	9.655885
7.182627	415.172084	9.660903
7.220486	407.922156	9.665920
7.724936	413.543851	9.670938
7.381979	421.049902	9.675955
7.809066	403.845525	9.680973
7.557410	398.064993	9.685991
7.222081	396.086952	9.691008
7.396374	382.292653	9.696026
7.278903	388.527831	9.701043
7.646360	387.503896	9.706061
7.615232	391.791855	9.711079
7.304135	378.300658	9.716096
7.696837	374.277032	9.721114
7.159029	376.831686	9.726131
7.191675	383.701461	9.731149
7.293214	383.004973	9.736167
7.282630	404.175109	9.741184
7.452077	398.521305	9.746202
7.262582	412.440680	9.751219
7.436752	417.176507	9.756237
7.032047	414.405276	9.761255
7.155578	414.201306	9.766272
7.956417	416.073626	9.771290
7.570529	420.838929	9.776307
7.850840	415.801014	9.781325
7.625804	416.899757	9.786343
7.764170	418.621865	9.791360
7.761356	419.087949	9.796378
7.481677	420.356614	9.801395
7.721227	418.542273	9.806413
7.635488	417.210436	9.811431
7.540186	413.461696	9.816448
7.964197	399.324013	9.821466
7.713453	402.369897	9.826483
7.340480	385.971036	9.831501
7.627372	385.637140	9.836519
7.400109	389.790617	9.841536
7.565898	401.800485	9.846554
7.786044	413.913659	9.851571
8.111725	412.707591	9.856589
7.708570	390.519666	9.861607
7.325344	386.147299	9.866624
7.212938	390.609382	9.871642
7.085253	409.768209	9.876659
7.539470	408.080270	9.881677
7.478084	418.339687	9.886695
7.547390	407.464659	9.891712
7.769354	419.695721	9.896730
7.674442	419.342654	9.901747
7.765321	417.572858	9.906765
8.050483	414.277178	9.911783
7.976949	419.175370	9.916800
8.086198	409.827766	9.921818
7.504488	418.289711	9.926835
7.515947	417.386107	9.931853
7.758667	413.321031	9.936871
7.759384	415.772625	9.941888
8.017010	419.906105	9.946906
7.689744	410.814456	9.951923
7.707895	417.794985	9.956941
7.514496	417.852204	9.961959
7.498278	419.008644	9.966976
7.891700	414.213400	9.971994
7.646293	411.564336	9.977011
7.543146	409.973326	9.982029
7.819387	413.015375	9.987047
7.469367	409.690538	9.992064
7.708891	413.018025	9.997082
7.733021	410.462580	10.002099
7.753045	420.506816	10.007117
8.119511	424.335363	10.012135
7.769143	421.695770	10.017152
7.813222	422.886332	10.022170
8.117848	433.485681	10.027187
7.834644	424.463596	10.032205
7.902249	418.240420	10.037223
7.997956	429.411480	10.042240
8.002748	407.666835	10.047258
7.774373	411.271208	10.052275
7.835275	420.308310	10.057293
8.064176	417.721681	10.062311
7.770384	430.006984	10.067328
7.995494	430.931066	10.072346
8.112339	433.042674	10.077363
8.195929	425.727811	10.082381
7.592264	414.658543	10.087399
7.661851	422.978714	10.092416
8.001496	425.814955	10.097434
8.189383	434.172066	10.102451
8.289423	429.366060	10.107469
8.236447	436.293109	10.112487
8.118093	422.013390	10.117504
8.249081	410.830297	10.122522
7.875979	417.435910	10.127539
7.798227	418.675929	10.132557
8.154752	416.034948	10.137575
7.993789	418.623770	10.142592
8.306150	411.919691	10.147610
8.069461	409.140868	10.152627
7.703553	419.200662	10.157645
8.068644	424.634412	10.162663
8.318801	435.299346	10.167680
8.571703	429.046429	10.172698
7.988329	415.623811	10.177715
7.822704	426.392973	10.182733
8.036374	407.645158	10.187751
8.238374	422.531714	10.192768
8.156584	425.903348	10.197786
8.381302	426.463988	10.202803
8.007422	429.144186	10.207821
8.282228	415.540289	10.212839
7.823471	414.755721	10.217856
8.179656	426.346333	10.222874
8.245321	429.602871	10.227891
8.005218	441.884331	10.232909
8.535035	436.667607	10.237927
8.477098	432.767836	10.242944
8.339720	417.484686	10.247962
8.078913	413.924187	10.252979
7.994127	411.627929	10.257997
8.283406	421.872795	10.263015
8.048458	430.491767	10.268032
8.458648	433.468584	10.273050
8.107984	430.798632	10.278067
8.425755	433.443452	10.283085
8.423720	432.249816	10.288103
8.137989	439.497456	10.293120
8.640927	430.825274	10.298138
8.632658	434.930174	10.303155
8.371537	416.213281	10.308173
8.379519	406.542328	10.313191
7.912882	399.990900	10.318208
8.282581	413.118213	10.323226
8.125660	435.900132	10.328243
8.146032	436.324991	10.333261
8.484741	433.244427	10.338279
8.168483	437.299163	10.343296
8.317648	432.071247	10.348314
8.325284	436.959869	10.353331
8.200458	440.462214	10.358349
8.351540	427.544853	10.363367
8.499197	440.711146	10.368384
8.403131	430.940862	10.373402
8.475747	430.524192	10.378419
8.424199	433.532441	10.383437
8.326184	433.097029	10.388455
8.204750	443.580416	10.393472
8.425009	433.353020	10.398490
8.446346	432.954073	10.403507
8.466591	439.473733	10.408525
8.503357	445.844830	10.413543
8.556628	432.629816	10.418560
8.393758	439.224707	10.423578
8.499500	430.087076	10.428595
8.562527	441.646241	10.433613
8.151432	436.591896	10.438631
8.076897	435.670422	10.443648
8.413818	434.182731	10.448666
8.641476	448.791508	10.453683
8.671120	453.033425	10.458701
8.637681	439.130028	10.463719
8.418535	446.455330	10.468736
8.590807	437.159978	10.473754
8.440615	452.298523	10.478771
8.728343	462.821568	10.483789
8.925703	455.070555	10.488807
8.583892	447.439546	10.493824
8.381201	433.819779	10.498842
8.777119	447.257682	10.503859
8.728474	461.497357	10.508877
8.949166	443.437170	10.513895
8.366864	435.087112	10.518912
8.354890	434.119579	10.523930
8.463826	442.951357	10.528947
8.453567	466.182805	10.533965
9.013389	467.342165	10.538983
8.724506	467.720808	10.544000
8.665447	463.926311	10.549018
9.120890	461.342386	10.554035
8.721598	470.782467	10.559053
8.850266	454.343046	10.564071
8.783257	463.072050	10.569088
9.010432	455.764540	10.574106
8.863647	436.233028	10.579123
8.538201	443.680401	10.584141
8.800054	433.116181	10.589159
8.726931	442.974981	10.594176
8.862952	433.736792	10.599194
8.734323	442.202599	10.604211
8.695904	455.623919	10.609229
8.831061	457.903827	10.614247
8.871874	469.307268	10.619264
9.032194	459.937713	10.624282
8.800099	439.828685	10.629299
8.716572	451.574838	10.634317
9.014638	451.378632	10.639335
8.636292	445.511069	10.644352
9.042761	465.930328	10.649370
9.000037	462.266667	10.654387
8.900930	454.711959	10.659405
9.208632	451.720159	10.664423
8.948171	432.800128	10.669440
8.740012	440.226247	10.674458
9.176373	430.826837	10.679475
8.509902	435.802159	10.684493
8.911401	453.702773	10.689511
9.078552	464.129135	10.694528
8.881651	454.497128	10.699546
8.765328	463.456774	10.704563
8.829861	463.962801	10.709581
9.199523	467.099243	10.714599
9.334013	461.618382	10.719616
8.887653	465.013173	10.724634
9.289513	451.264751	10.729651
8.839001	455.848264	10.734669
8.667155	461.367413	10.739687
8.847516	462.944327	10.744704
8.898898	464.713387	10.749722
9.269162	465.343363	10.754739
9.115402	472.170670	10.759757
9.115751	468.480700	10.764775
9.093334	480.146121	10.769792
9.038316	471.824336	10.774810
9.272123	461.965175	10.779827
8.968892	465.261526	10.784845
8.995424	466.402639	10.789863
9.170645	472.418357	10.794880
8.802237	465.847518	10.799898
9.146600	460.261321	10.804915
8.946965	466.414656	10.809933
9.238503	472.921578	10.814951
9.099188	468.706967	10.819968
8.766544	464.571836	10.824986
8.790006	474.032492	10.830003
9.082767	470.550051	10.835021
8.869931	459.860068	10.840039
9.146357	474.588638	10.845056
9.113299	483.714124	10.850074
9.319295	487.762571	10.855091
9.447653	497.473863	10.860109
9.426247	476.981813	10.865127
9.296632	470.830765	10.870144
9.039580	469.553901	10.875162
9.384995	468.277751	10.880179
9.203542	476.390768	10.885197
9.166196	477.499337	10.890215
9.454657	484.520740	10.895232
9.405833	492.970828	10.900250
9.449237	470.940734	10.905267
9.136792	471.768749	10.910285
9.109188	472.630287	10.915303
9.651758	483.983196	10.920320
9.355633	484.805366	10.925338
9.451951	479.419765	10.930355
9.326753	486.674454	10.935373
9.388607	481.031315	10.940391
9.349610	477.942210	10.945408
9.296801	486.847878	10.950426
9.522888	479.754174	10.955443
9.507107	492.052135	10.960461
9.502208	489.775432	10.965479
9.615885	484.565664	10.970496
9.421878	469.431456	10.975514
9.380355	465.702353	10.980531
9.061812	473.058559	10.985549
9.204276	479.739891	10.990567
9.268512	480.057424	10.995584
9.203013	485.541589	11.000602
9.486962	482.332790	11.005619
9.450036	501.944254	11.010637
9.520016	490.209983	11.015655
9.811336	487.955278	11.020672
9.710893	491.835121	11.025690
9.507825	474.000702	11.030707
9.574309	498.187621	11.035725
9.785605	486.708288	11.040743
9.544505	491.088048	11.045760
9.270480	495.908789	11.050778
9.755509	479.763823	11.055795
9.571169	486.666943	11.060813
9.506583	486.620609	11.065831
9.715447	487.599140	11.070848
9.588916	488.578482	11.075866
9.593614	489.624701	11.080883
9.635832	484.703850	11.085901
9.180406	487.480095	11.090919
9.534537	481.609854	11.095936
9.449163	492.963314	11.100954
9.791228	489.745106	11.105971
9.301349	497.828214	11.110989
9.452561	489.819215	11.116007
9.946974	505.552029	11.121024
9.493636	508.034293	11.126042
10.289721	506.756485	11.131059
9.671350	496.426640	11.136077
9.494163	493.927574	11.141095
9.625816	489.076275	11.146112
9.699222	511.070202	11.151130
9.742561	514.499507	11.156147
9.993291	517.918945	11.161165
9.925010	517.569052	11.166183
9.927079	491.496296	11.171200
9.583234	491.569324	11.176218
9.945915	500.500807	11.181235
10.007837	515.490212	11.186253
9.904440	502.312443	11.191271
9.955859	485.205777	11.196288
9.451523	489.033885	11.201306
9.600363	502.641578	11.206323
9.965750	517.680717	11.211341
9.976288	506.529957	11.216359
9.971086	511.092347	11.221376
9.860234	519.737505	11.226394
10.125347	522.897435	11.231411
10.108424	518.901906	11.236429
9.778311	508.216804	11.241447
9.839024	511.480574	11.246464
9.782838	517.687669	11.251482
10.074484	521.159980	11.256499
10.224111	517.786992	11.261517
9.823053	516.978122	11.266535
10.226956	518.640124	11.271552
10.072839	519.785607	11.276570
10.378303	520.027261	11.281587
9.869998	503.072509	11.286605
9.800942	493.050627	11.291623
10.114805	495.878645	11.296640
10.249924	513.051167	11.301658
10.080923	499.423806	11.306675
9.903146	495.106413	11.311693
10.010122	520.627147	11.316711
10.013745	516.284003	11.321728
10.182786	528.634603	11.326746
10.424580	519.754988	11.331763
10.370967	522.064231	11.336781
9.927512	497.926027	11.341799
9.983540	503.025328	11.346816
10.205411	513.964031	11.351834
10.016525	517.546453	11.356851
10.096182	520.658405	11.361869
10.040459	513.563135	11.366887
10.289739	528.751170	11.371904
9.968461	523.500888	11.376922
10.264576	525.307350	11.381939
10.083488	522.177655	11.386957
10.360686	525.691422	11.391975
10.549592	507.304295	11.396992
10.240116	519.581044	11.402010
10.544880	514.982863	11.407027
10.495804	516.796378	11.412045
10.517545	517.062876	11.417063
10.364966	499.289065	11.422080
9.870224	506.922582	11.427098
10.321525	505.674395	11.432115
10.478458	516.752249	11.437133
10.220654	519.324420	11.442151
10.566596	514.061695	11.447168
10.519291	512.235606	11.452186
9.947719	510.589246	11.457203
10.232443	510.515299	11.462221
10.446911	525.174252	11.467239
10.592350	516.503140	11.472256
10.434420	522.627858	11.477274
10.412327	520.563497	11.482291
10.131366	509.094249	11.487309
10.172928	519.522608	11.492327
10.267513	512.617810	11.497344
10.144963	529.097353	11.502362
10.261253	526.469583	11.507379
10.398393	518.408871	11.512397
10.199304	528.199682	11.517415
10.359723	526.019054	11.522432
10.196011	528.303687	11.527450
10.356523	521.676710	11.532467
10.305344	523.168297	11.537485
10.360257	538.729435	11.542503
10.491743	540.990084	11.547520
10.739746	547.427082	11.552538
10.940824	551.591887	11.557555
10.741793	538.802552	11.562573
10.453182	531.268987	11.567591
10.724536	518.754520	11.572608
10.629702	526.734769	11.577626
10.480225	520.371477	11.582643
10.360800	528.606527	11.587661
10.667760	541.417219	11.592679
10.841512	539.772171	11.597696
10.312874	543.892143	11.602714
10.476107	545.583488	11.607731
10.818323	545.967858	11.612749
10.857725	550.576618	11.617767
11.046481	546.455182	11.622784
10.672729	536.651700	11.627802
10.709691	526.296691	11.632819
10.965752	534.401695	11.637837
10.601603	524.401989	11.642855
10.738237	517.427359	11.647872
10.753442	520.419476	11.652890
10.608384	533.837920	11.657907
10.968026	546.099864	11.662925
10.580511	547.896787	11.667943
11.046192	546.876192	11.672960
10.692887	542.457603	11.677978
10.470788	549.628159	11.682995
10.954126	540.195334	11.688013
10.720385	554.158756	11.693031
10.913786	536.299388	11.698048
10.867153	546.534606	11.703066
10.667140	544.962738	11.708083
10.913063	540.516566	11.713101
10.935934	545.609848	11.718119
10.964759	546.785325	11.723136
11.193642	549.813875	11.728154
10.921909	550.202183	11.733171
10.844556	543.180539	11.738189
11.228573	557.429987	11.743207
10.973576	542.031236	11.748224
10.979814	554.141787	11.753242
10.918989	544.568026	11.758259
11.266335	541.806815	11.763277
10.977042	546.310869	11.768295
11.450835	537.465429	11.773312
10.981402	529.875445	11.778330
10.692808	526.781720	11.783347
11.244736	533.531012	11.788365
11.053085	539.866484	11.793383
11.168498	542.715399	11.798400
10.972435	537.711393	11.803418
11.158583	521.749605	11.808435
10.841329	530.498056	11.813453
11.232601	545.718931	11.818471
11.226330	540.735222	11.823488
11.218138	546.318972	11.828506
11.114704	541.649094	11.833523
10.962091	525.522167	11.838541
11.344092	540.753917	11.843559
11.229424	543.535068	11.848576
11.060515	538.540450	11.853594
11.140131	535.015970	11.858611
10.995236	540.849231	11.863629
10.792414	552.148045	11.868647
10.792771	544.777897	11.873664
11.150856	547.596452	11.878682
11.043949	551.540062	11.883699
10.923226	547.066209	11.888717
10.969453	557.127361	11.893735
11.256144	556.147268	11.898752
10.971560	557.822676	11.903770
11.073607	571.670794	11.908787
11.571670	579.966296	11.913805
11.607421	584.366262	11.918823
11.666242	568.486085	11.923840
11.401261	554.335078	11.928858
11.328009	553.381600	11.933875
11.306571	549.047803	11.938893
11.362572	551.635924	11.943911
11.339044	549.513244	11.948928
11.239141	543.480953	11.953946
11.217553	550.220915	11.958963
11.344857	562.329081	11.963981
11.686102	570.087318	11.968999
11.747865	563.945938	11.974016
11.573590	549.057651	11.979034
11.524944	550.378581	11.984051
11.750304	541.997533	11.989069
11.311569	537.181926	11.994087
11.351978	545.210293	11.999104
11.359302	540.204165	12.004122
11.394664	554.126660	12.009139
11.621502	549.089174	12.014157
11.407001	548.572537	12.019175
11.586174	565.990247	12.024192
11.859912	566.773848	12.029210
11.704287	559.356060	12.034227
11.772195	550.122858	12.039245
11.333956	554.603802	12.044263
11.289406	545.094168	12.049280
11.732703	557.413739	12.054298
11.592117	571.711121	12.059315
11.895699	572.256373	12.064333
11.759236	559.571520	12.069351
11.488233	554.863594	12.074368
11.797112	555.676813	12.079386
11.507619	572.765271	12.084403
11.541405	571.050750	12.089421
11.734423	572.435170	12.094439
11.625693	582.807223	12.099456
11.900468	575.798520	12.104474
11.610876	580.275671	12.109491
11.644347	574.253505	12.114509
11.759884	588.717591	12.119527
11.731034	575.995063	12.124544
11.907178	571.046443	12.129562
11.763702	581.269150	12.134579
11.737508	579.516026	12.139597
11.723599	576.055801	12.144615
11.754698	574.106732	12.149632
11.748655	586.642383	12.154650
11.237459	578.207872	12.159667
11.698196	577.183271	12.164685
11.661583	579.732184	12.169703
11.614328	585.644780	12.174720
12.220385	576.899188	12.179738
11.633558	581.291430	12.184755
11.814722	581.496748	12.189773
12.041338	580.464586	12.194791
12.112326	587.621758	12.199808
12.039998	578.568473	12.204826
11.948838	582.416988	12.209843
12.013927	576.179402	12.214861
12.087922	578.621079	12.219879
11.948948	581.542938	12.224896
12.013912	579.482682	12.229914
11.865469	593.722537	12.234931
12.014211	581.004115	12.239949
11.915797	597.120071	12.244967
12.120322	606.909673	12.249984
12.774939	600.993667	12.255002
12.390937	593.635547	12.260019
12.235752	579.648816	12.265037
12.149669	583.460377	12.270055
11.728517	583.424551	12.275072
11.893458	567.376671	12.280090
11.816310	576.951733	12.285107
12.080907	593.498443	12.290125
11.988435	596.305359	12.295143
12.454658	605.632408	12.300160
12.791197	595.324087	12.305178
12.336567	595.287200	12.310195
12.464868	575.418869	12.315213
12.499981	579.828190	12.320231
12.249477	571.495259	12.325248
12.320669	575.152507	12.330266
12.047910	577.411967	12.335283
12.183230	575.141896	12.340301
12.297811	576.540263	12.345319
11.976003	576.873474	12.350336
12.364983	567.337746	12.355354
12.336374	582.322101	12.360371
12.231810	579.363964	12.365389
12.468413	593.506731	12.370407
12.209437	592.587288	12.375424
12.187165	595.578430	12.380442
12.356871	605.647746	12.385459
12.450898	606.927095	12.390477
12.597600	595.864967	12.395495
12.418962	613.425112	12.400512
12.970387	603.080586	12.405530
12.377275	587.802808	12.410547
12.333551	574.329347	12.415565
12.434120	585.633845	12.420583
12.280082	596.547146	12.425600
12.566823	593.739751	12.430618
12.487808	597.688899	12.435635
12.515901	592.478575	12.440653
12.518460	591.502332	12.445671
12.749409	594.753340	12.450688
12.867113	592.217727	12.455706
12.370193	576.025426	12.460723
12.352536	588.773193	12.465741
12.233817	599.126144	12.470759
12.282672	596.432356	12.475776
12.576250	595.228825	12.480794
12.698651	605.037606	12.485811
12.677286	598.360452	12.490829
13.143777	588.622275	12.495847
12.654314	594.944497	12.500864
12.740356	588.384019	12.505882
12.190967	589.644720	12.510899
12.404063	593.626287	12.515917
12.528461	600.406700	12.520935
12.685992	607.869398	12.525952
13.112389	590.452075	12.530970
12.724134	593.524264	12.535987
12.367303	594.285029	12.541005
12.539576	597.752778	12.546023
12.202123	600.098016	12.551040
12.656889	614.822343	12.556058
12.901560	628.225569	12.561075
13.045760	628.771379	12.566093
13.300320	617.462126	12.571111
12.712083	602.931902	12.576128
13.070534	596.429239	12.581146
12.964288	596.178413	12.586163
13.180981	589.448245	12.591181
12.928848	587.249778	12.596199
12.813326	602.011555	12.601216
12.771913	582.962343	12.606234
12.994371	590.306746	12.611251
12.884091	590.903760	12.616269
13.037738	597.552297	12.621287
13.062797	596.141714	12.626304
13.003167	599.270204	12.631322
13.082455	594.967968	12.636339
12.936355	587.631646	12.641357
13.160379	608.074160	12.646375
12.777348	597.807993	12.651392
13.035666	596.754649	12.656410
13.213069	598.992466	12.661427
12.738567	596.365189	12.666445
13.236720	593.363243	12.671463
13.309299	610.072583	12.676480
13.260459	612.485558	12.681498
13.039115	597.612088	12.686515
12.842006	595.306515	12.691533
13.245932	601.728692	12.696551
13.421841	618.829349	12.701568
13.133215	594.723169	12.706586
12.951055	602.944615	12.711603
13.266406	614.371975	12.716621
13.272000	615.017643	12.721639
13.550517	625.950312	12.726656
13.568948	610.975209	12.731674
13.269956	595.395523	12.736691
12.873907	598.951384	12.741709
13.275275	595.373327	12.746727
13.347427	623.574452	12.751744
13.264016	620.466679	12.756762
13.644580	621.294329	12.761779
13.326554	610.948231	12.766797
13.165567	603.518712	12.771815
12.941148	615.635546	12.776832
13.280361	615.790637	12.781850
13.281889	624.352236	12.786867
13.361128	623.154011	12.791885
13.302313	628.398883	12.796903
13.704685	628.563316	12.801920
13.556587	625.210475	12.806938
13.231125	620.548628	12.811955
13.121241	632.987622	12.816973
13.389698	618.646848	12.821991
13.202778	633.122973	12.827008
13.608076	617.848842	12.832026
13.589573	611.300219	12.837043
13.507835	619.374986	12.842061
13.726856	617.412175	12.847079
13.409179	632.058205	12.852096
13.499052	620.171462	12.857114
13.734689	623.977299	12.862131
13.506891	625.421425	12.867149
13.456533	623.275911	12.872167
13.545869	622.251278	12.877184
13.471888	624.155223	12.882202
13.713668	614.985554	12.887219
13.613919	626.423657	12.892237
13.649568	617.899149	12.897255
13.676482	614.474878	12.902272
13.208812	622.867999	12.907290
13.974549	626.600111	12.912307
13.654486	631.782272	12.917325
13.760476	626.100984	12.922343
14.185324	639.106605	12.927360
13.755655	637.612828	12.932378
13.752768	624.471583	12.937395
13.628370	625.246093	12.942413
13.863764	614.107103	12.947431
13.911179	628.907125	12.952448
13.870312	623.387088	12.957466
14.100575	625.286515	12.962483
13.774568	623.204265	12.967501
14.217415	617.392034	12.972519
13.752889	620.062445	12.977536
13.872694	622.958868	12.982554
13.834047	609.607052	12.987571
13.978610	618.376953	12.992589
13.904494	624.952238	12.997607
13.939364	612.343731	13.002624
13.769441	627.862997	13.007642
14.205644	630.523608	13.012659
14.077996	635.423727	13.017677
13.988263	628.017453	13.022695
13.954150	634.753716	13.027712
14.041267	635.656529	13.032730
14.291509	644.927677	13.037747
13.973966	643.738536	13.042765
14.038707	629.576368	13.047783
14.214244	638.629294	13.052800
14.358152	640.416837	13.057818
14.011215	626.659350	13.062835
13.659801	616.018629	13.067853
14.202473	635.848102	13.072871
14.123244	638.367362	13.077888
14.420319	644.789895	13.082906
14.459297	643.982104	13.087923
14.418739	647.083639	13.092941
14.438567	640.359509	13.097959
14.122300	623.199793	13.102976
13.937005	622.291691	13.107994
14.416910	629.399807	13.113011
13.911596	644.262351	13.118029
14.423385	642.618210	13.123047
14.246891	644.963621	13.128064
14.432230	637.410725	13.133082
14.575470	637.020068	13.138099
14.700660	644.677362	13.143117
14.253256	621.562544	13.148135
13.846787	622.720510	13.153152
14.051471	638.651999	13.158170
14.665631	629.285477	13.163187
14.463226	646.166257	13.168205
14.406070	642.674786	13.173223
14.108425	635.263308	13.178240
14.250393	642.221214	13.183258
14.575229	640.557387	13.188275
14.531150	650.270111	13.193293
14.344122	637.313782	13.198311
14.608995	634.307967	13.203328
14.407628	641.163291	13.208346
14.774904	642.508391	13.213363
14.265394	652.562054	13.218381
14.733093	633.821482	13.223399
14.729315	639.256337	13.228416
14.375816	638.949736	13.233434
14.991923	636.842972	13.238451
14.721242	635.469251	13.243469
14.851457	630.726883	13.248487
14.888123	642.833067	13.253504
14.715210	634.011487	13.258522
15.131946	637.139890	13.263539
14.879965	640.449851	13.268557
14.740807	624.348446	13.273575
15.148613	638.615294	13.278592
14.352295	622.889562	13.283610
14.662790	634.341652	13.288627
14.639734	641.869832	13.293645
14.822712	639.490420	13.298663
14.811267	631.658788	13.303680
14.634052	642.114527	13.308698
14.872292	631.611149	13.313715
14.366038	640.559563	13.318733
14.890861	630.971038	13.323751
14.550249	628.205510	13.328768
14.478348	631.743632	13.333786
14.676630	630.101113	13.338803
14.493550	630.303645	13.343821
14.663368	651.531498	13.348839
14.967735	660.624848	13.353856
14.899160	666.938164	13.358874
15.058303	659.997833	13.363891
15.126088	667.224554	13.368909
15.108853	665.613316	13.373927
15.223334	661.264210	13.378944
14.885621	673.405519	13.383962
15.189136	658.748640	13.388979
15.413357	667.092986	13.393997
14.731056	658.057597	13.399015
15.154423	650.821786	13.404032
14.809828	661.586836	13.409050
15.033991	659.491503	13.414067
15.040535	661.729519	13.419085
15.160469	653.105942	13.424103
15.444081	670.039379	13.429120
15.311489	662.172251	13.434138
15.356043	649.726648	13.439155
15.182166	662.940461	13.444173
15.265235	671.412544	13.449191
15.613821	667.262105	13.454208
15.016200	671.565327	13.459226
15.384532	660.784870	13.464243
15.561584	660.685417	13.469261
15.315943	661.086932	13.474279
15.526664	658.145168	13.479296
14.961556	650.192957	13.484314
15.192259	644.089853	13.489331
15.277953	665.174964	13.494349
15.658219	659.759991	13.499367
15.267171	668.810324	13.504384
15.067046	669.475524	13.509402
15.575998	661.447567	13.514419
15.429550	661.652804	13.519437
15.281805	661.432453	13.524455
15.652214	658.830862	13.529472
15.647158	663.011359	13.534490
15.634912	656.872823	13.539507
15.559482	661.768650	13.544525
15.473467	654.789126	13.549543
15.967200	662.005187	13.554560
15.513229	657.290466	13.559578
15.871598	659.372230	13.564595
15.177433	658.422062	13.569613
15.086968	657.068745	13.574631
16.016186	653.652314	13.579648
15.613278	658.179702	13.584666
15.729089	657.239454	13.589683
15.662044	665.701505	13.594701
15.524531	662.736692	13.599719
15.639020	664.757303	13.604736
15.758831	668.920907	13.609754
15.822201	660.186520	13.614771
15.725204	663.306831	13.619789
15.679419	663.959909	13.624807
15.950349	661.829688	13.629824
15.883259	659.990417	13.634842
16.022390	658.170109	13.639859
15.830489	663.919371	13.644877
16.026327	658.486952	13.649895
15.936411	650.558359	13.654912
15.802317	668.413607	13.659930
15.960453	661.883204	13.664947
16.014163	669.221187	13.669965
15.693794	660.983003	13.674983
16.016453	654.964679	13.680000
15.519819	663.050662	13.685018
15.863548	662.431537	13.690035
16.008185	660.564461	13.695053
15.921477	663.726667	13.700071
15.794894	653.453312	13.705088
15.726830	665.052907	13.710106
15.475820	665.773751	13.715123
15.906387	656.403011	13.720141
15.779184	679.290792	13.725159
16.162666	670.759552	13.730176
16.046170	685.557685	13.735194
16.328681	689.008616	13.740211
16.414980	691.152075	13.745229
16.188730	680.357580	13.750247
16.189613	657.037549	13.755264
15.887037	673.042273	13.760282
16.543921	688.593340	13.765299
16.622554	678.745415	13.770317
16.075057	663.244514	13.775335
16.080536	659.439598	13.780352
16.362697	667.249079	13.785370
16.252825	663.875741	13.790387
16.237746	660.114274	13.795405
16.117925	671.657283	13.800423
16.632856	674.831266	13.805440
16.286964	672.563947	13.810458
16.698914	675.772071	13.815475
16.304309	659.423626	13.820493
16.184172	664.904978	13.825511
16.637656	670.420351	13.830528
16.217676	663.489222	13.835546
16.514571	668.593353	13.840563
16.415888	677.936747	13.845581
16.174725	685.428958	13.850599
16.729945	690.406270	13.855616
16.454814	690.825943	13.860634
16.609744	691.069155	13.865651
16.688612	677.516104	13.870669
16.652104	680.701114	13.875687
16.475290	675.394333	13.880704
16.670843	685.387594	13.885722
16.983415	675.194182	13.890739
16.657596	671.223976	13.895757
16.311400	659.209008	13.900775
16.501123	663.999122	13.905792
16.342698	682.511035	13.910810
16.603685	688.267044	13.915827
16.755220	681.532350	13.920845
16.438273	688.525079	13.925863
16.786475	680.811908	13.930880
16.744568	690.583637	13.935898
16.722006	686.835898	13.940915
16.667048	674.111698	13.945933
16.507124	675.434693	13.950951
16.579711	673.629807	13.955968
16.476973	685.927238	13.960986
16.696399	681.760942	13.966003
16.945235	682.162322	13.971021
16.881752	686.182435	13.976039
16.942557	685.641849	13.981056
16.967429	683.876239	13.986074
16.929337	682.443609	13.991091
17.172114	681.499894	13.996109
16.942266	680.938553	14.001127
16.994117	683.916184	14.006144
16.840364	674.931012	14.011162
16.890032	679.142326	14.016179
17.194576	684.302863	14.021197
16.869292	694.515935	14.026215
17.065801	685.354590	14.031232
17.084023	684.094706	14.036250
16.847778	682.539832	14.041267
16.998062	696.203452	14.046285
17.127065	720.098358	14.051303
17.515870	710.683905	14.056320
17.177327	725.832196	14.061338
17.469093	711.434541	14.066355
16.999843	687.913665	14.071373
16.949918	707.918606	14.076391
17.466284	703.339032	14.081408
17.399230	711.654190	14.086426
17.151718	701.967114	14.091443
17.022133	707.565866	14.096461
17.469945	711.471479	14.101479
17.488891	701.617068	14.106496
17.324863	717.450743	14.111514
17.307538	708.001457	14.116531
17.652024	709.112089	14.121549
17.707832	706.730852	14.126567
17.273867	687.806899	14.131584
17.096652	694.432414	14.136602
17.548782	701.683907	14.141619
17.637718	704.458700	14.146637
17.180689	707.880104	14.151655
17.276489	707.273116	14.156672
17.307100	713.720818	14.161690
16.951575	706.746839	14.166707
17.835129	710.163890	14.171725
17.449680	713.116567	14.176743
17.500891	708.449915	14.181760
17.358290	710.322207	14.186778
17.237213	698.562962	14.191795
17.749392	701.924378	14.196813
17.458675	706.974966	14.201831
17.461183	704.801023	14.206848
17.422081	705.856267	14.211866
17.163848	711.934164	14.216883
17.983615	709.914578	14.221901
18.198105	731.892789	14.226919
18.131294	710.169979	14.231936
17.712755	704.718130	14.236954
17.706353	705.994699	14.241971
18.064259	702.882568	14.246989
17.975114	705.109735	14.252007
17.859177	693.857519	14.257024
17.981156	695.537100	14.262042
17.798965	711.135922	14.267059
17.759938	704.739835	14.272077
17.933018	711.140277	14.277095
18.032410	704.613955	14.282112
18.039457	695.401843	14.287130
17.664805	712.301910	14.292147
18.031581	707.394564	14.297165
17.691349	696.867173	14.302183
17.936904	704.634601	14.307200
17.846138	693.846245	14.312218
17.944169	714.902226	14.317235
18.468193	717.226847	14.322253
18.039392	710.575349	14.327271
18.247231	700.200349	14.332288
18.116539	694.874131	14.337306
18.061211	704.562474	14.342323
18.216148	690.600264	14.347341
17.897936	698.550009	14.352359
18.271969	714.549735	14.357376
18.357606	712.913719	14.362394
18.275541	719.246212	14.367411
18.284294	705.377325	14.372429
18.344885	702.927693	14.377447
18.293239	700.497397	14.382464
18.307129	696.708401	14.387482
18.194504	704.842638	14.392499
18.526710	708.132240	14.397517
18.549702	700.602599	14.402535
18.171084	702.613775	14.407552
18.371994	699.389329	14.412570
18.380148	715.617006	14.417587
18.616846	718.142328	14.422605
18.493873	714.838651	14.427623
18.193740	707.197967	14.432640
18.449560	711.217969	14.437658
18.525063	723.499062	14.442675
18.506802	719.295573	14.447693
18.434023	713.952496	14.452711
18.371814	714.925552	14.457728
18.450516	713.268540	14.462746
18.290952	730.632791	14.467763
18.514702	725.979149	14.472781
18.373171	720.964595	14.477799
18.394311	711.136975	14.482816
18.785973	714.305653	14.487834
18.306330	713.703815	14.492851
18.698413	708.896204	14.497869
18.698309	712.274870	14.502887
18.524013	710.167833	14.507904
18.731565	709.162430	14.512922
18.561159	713.602308	14.517939
18.768678	716.633930	14.522957
18.569246	721.826495	14.527975
18.736147	729.296068	14.532992
18.956700	742.248448	14.538010
19.002355	748.553450	14.543027
19.326770	732.067115	14.548045
18.871220	726.061541	14.553063
19.194756	714.735406	14.558080
18.990221	710.432214	14.563098
18.675166	715.349157	14.568115
19.266071	709.975229	14.573133
19.001867	721.428870	14.578151
18.531949	707.207276	14.583168
19.058109	712.200222	14.588186
19.145864	718.680504	14.593203
19.212052	715.567080	14.598221
19.083257	717.415344	14.603239
19.024381	718.281571	14.608256
19.143417	709.905897	14.613274
19.138447	712.841457	14.618291
19.146274	705.957109	14.623309
19.137726	713.833548	14.628327
19.216351	721.546303	14.633344
19.533968	725.089552	14.638362
19.233773	722.007151	14.643379
19.364602	712.192500	14.648397
19.411530	713.856735	14.653415
19.057519	712.558183	14.658432
19.161449	712.236115	14.663450
19.243109	724.600625	14.668467
19.455551	730.861919	14.673485
19.180912	727.338862	14.678503
19.281863	741.579857	14.683520
19.732728	736.560200	14.688538
19.767965	741.581733	14.693555
19.533161	725.077603	14.698573
19.184892	724.171038	14.703591
19.020935	737.502249	14.708608
19.311079	734.979153	14.713626
19.497293	740.303922	14.718643
19.738726	733.105616	14.723661
19.640502	746.057342	14.728679
20.062512	745.040705	14.733696
19.741285	734.901213	14.738714
19.350204	735.695100	14.743731
19.827705	736.256983	14.748749
19.466518	742.320021	14.753767
19.616494	735.238974	14.758784
19.770056	740.268901	14.763802
19.653885	734.633930	14.768819
19.844047	732.541549	14.773837
19.756320	730.864803	14.778855
19.325940	733.937485	14.783872
19.998890	733.937840	14.788890
19.806829	736.414652	14.793907
19.417207	736.911306	14.798925
19.524043	741.916678	14.803943
19.346248	739.367780	14.808960
19.305948	738.728075	14.813978
19.532185	749.608067	14.818995
19.959235	758.022271	14.824013
20.011845	761.445081	14.829031
19.830187	768.896305	14.834048
20.130679	755.959685	14.839066
20.106113	762.584113	14.844083
20.092987	763.041972	14.849101
20.208544	764.085242	14.854119
20.259353	765.133308	14.859136
20.379854	755.335786	14.864154
20.148458	745.790382	14.869171
20.120757	738.503012	14.874189
19.803548	737.428942	14.879207
19.947784	761.056780	14.884224
20.483767	752.450008	14.889242
20.457194	762.274160	14.894259
20.069034	757.204502	14.899277
20.391681	757.754877	14.904295
20.132060	755.243706	14.909312
20.070382	766.417010	14.914330
20.095794	758.410849	14.919347
20.000435	770.211552	14.924365
20.512727	763.364066	14.929383
20.278895	767.716034	14.934400
20.563899	766.921901	14.939418
20.063999	771.164620	14.944435
20.315055	765.179539	14.949453
20.570991	754.989726	14.954471
20.122966	765.813567	14.959488
20.404441	760.794930	14.964506
20.385524	758.859810	14.969523
20.300022	756.203647	14.974541
20.258552	754.306007	14.979559
20.089249	758.669353	14.984576
20.788917	769.395350	14.989594
20.986696	780.807723	14.994611
20.695322	770.257150	14.999629
20.534577	757.345972	15.004647
20.388471	760.856039	15.009664
20.744242	768.484247	15.014682
20.874588	789.232291	15.019699
20.798596	779.025871	15.024717
20.780302	776.148205	15.029735
20.559378	769.557093	15.034752
20.886129	776.651718	15.039770
20.638535	784.947645	15.044787
20.854399	791.768923	15.049805
20.990164	781.336599	15.054823
20.944773	796.385737	15.059840
21.482913	778.929857	15.064858
20.824995	765.616868	15.069875
20.672235	747.784739	15.074893
20.968027	757.603737	15.079911
20.999984	773.497290	15.084928
21.337562	776.789464	15.089946
21.303117	764.566134	15.094963
20.833938	755.277201	15.099981
21.273637	745.329122	15.104999
20.700518	742.945630	15.110016
20.675226	746.523410	15.115034
21.131516	760.565276	15.120051
21.171363	767.376170	15.125069
21.241362	768.858187	15.130087
21.089499	778.059573	15.135104
21.459051	773.104611	15.140122
21.566627	778.585767	15.145139
21.162868	771.783772	15.150157
20.947190	776.384861	15.155175
20.938201	784.292702	15.160192
21.226459	772.986229	15.165210
21.119304	780.006721	15.170227
20.946176	784.262458	15.175245
21.446635	776.843900	15.180263
21.159569	785.605515	15.185280
21.379896	776.733630	15.190298
21.351297	781.971100	15.195315
21.245517	774.786755	15.200333
21.371561	774.776720	15.205351
21.178449	786.020862	15.210368
21.565731	780.681445	15.215386
21.562450	784.885005	15.220403
21.474697	790.106176	15.225421
21.895931	791.706202	15.230439
21.547584	786.444754	15.235456
21.460023	786.109947	15.240474
21.669307	791.417243	15.245491
21.419397	791.575910	15.250509
21.597432	796.376262	15.255527
21.921039	805.526449	15.260544
22.137380	797.749396	15.265562
21.913606	788.933868	15.270579
21.782359	781.094403	15.275597
22.134252	776.578300	15.280615
22.081584	783.191242	15.285632
22.070955	781.461010	15.290650
21.902644	780.808704	15.295667
21.896091	771.785176	15.300685
21.878086	769.266942	15.305703
21.771462	774.366545	15.310720
21.764306	773.275186	15.315738
22.060379	764.964501	15.320755
21.492606	774.895907	15.325773
21.745280	772.363252	15.330791
21.799932	782.742785	15.335808
21.966186	789.920621	15.340826
22.079241	798.107557	15.345843
21.663767	798.526610	15.350861
22.202775	794.274998	15.355879
22.100994	804.160022	15.360896
22.112781	797.814640	15.365914
22.242373	791.951472	15.370931
22.055242	797.163974	15.375949
22.007712	796.152795	15.380967
22.245543	798.085731	15.385984
21.852105	794.784614	15.391002
22.093930	787.476101	15.396019
22.152109	796.181359	15.401037
22.058228	791.702506	15.406055
22.268314	815.894734	15.411072
22.426178	820.313165	15.416090
22.788807	817.557449	15.421107
22.695717	816.984918	15.426125
22.308132	802.581846	15.431143
22.394758	806.307157	15.436160
22.665848	813.041184	15.441178
22.714125	805.962444	15.446195
22.659316	815.341479	15.451213
22.733013	791.919561	15.456231
22.669750	797.996960	15.461248
22.164542	793.844004	15.466266
22.170585	803.220650	15.471283
22.716291	826.947570	15.476301
23.093940	810.686365	15.481319
22.778325	827.766827	15.486336
22.834780	812.445740	15.491354
22.847237	797.428537	15.496371
22.558454	804.164054	15.501389
22.574472	807.679126	15.506407
22.812392	822.719063	15.511424
22.928307	827.370469	15.516442
23.020998	822.864515	15.521459
22.835189	826.551402	15.526477
23.435487	825.947440	15.531495
23.200392	823.275541	15.536512
22.775321	808.402369	15.541530
23.138813	793.332671	15.546547
22.733652	788.171931	15.551565
22.815786	803.808451	15.556583
22.986935	794.958459	15.561600
22.969804	788.403924	15.566618
22.717542	796.590512	15.571635
22.893327	822.187665	15.576653
23.022096	818.210395	15.581671
22.941841	819.407364	15.586688
23.098270	829.349420	15.591706
23.211399	821.793310	15.596723
23.069010	830.195573	15.601741
23.082355	815.430324	15.606759
23.298279	823.759103	15.611776
23.297052	829.476622	15.616794
23.325148	820.115314	15.621811
22.950118	828.639766	15.626829
23.086009	825.835707	15.631847
23.144447	823.459429	15.636864
23.153997	823.854498	15.641882
23.635868	814.780836	15.646899
23.455495	815.812297	15.651917
23.284171	816.851708	15.656935
23.449757	830.946501	15.661952
23.491431	839.774174	15.666970
23.906729	851.333199	15.671987
23.461232	841.564896	15.677005
23.639046	832.506830	15.682023
23.493179	840.117891	15.687040
23.698583	847.160469	15.692058
23.603754	843.639160	15.697075
23.787443	858.379194	15.702093
23.329655	849.687917	15.707111
23.489736	850.907070	15.712128
23.732851	853.292304	15.717146
24.158089	848.675100	15.722163
23.649239	848.118035	15.727181
24.132374	843.990090	15.732199
24.121592	848.870570	15.737216
24.119633	849.158212	15.742234
23.776012	831.144572	15.747251
24.310966	839.745087	15.752269
23.944720	826.980781	15.757287
23.878734	825.220132	15.762304
23.371929	818.694939	15.767322
23.863001	828.380452	15.772339
23.554837	845.176979	15.777357
23.937670	831.751973	15.782375
24.384673	840.577023	15.787392
24.080149	840.849124	15.792410
24.384794	843.005529	15.797427
24.064066	837.043859	15.802445
23.902735	842.721318	15.807463
24.043608	834.602944	15.812480
23.987073	841.650525	15.817498
23.878885	838.749815	15.822515
23.897703	848.550678	15.827533
23.666519	858.137593	15.832551
24.179014	862.163241	15.837568
24.098113	869.123244	15.842586
24.361099	882.236613	15.847603
24.256765	875.092133	15.852621
24.278513	869.765461	15.857639
24.201549	871.717264	15.862656
24.507417	877.762331	15.867674
24.488490	879.830800	15.872691
24.568859	877.087472	15.877709
24.594931	886.426614	15.882727
24.860044	862.022934	15.887744
24.545739	872.328582	15.892762
24.866274	873.859644	15.897779
25.012341	868.718887	15.902797
24.741636	871.186181	15.907815
25.058445	873.896483	15.912832
24.959956	868.900156	15.917850
25.299140	855.574353	15.922867
25.113199	841.432455	15.927885
24.700803	840.047888	15.932903
24.864657	834.276858	15.937920
24.600110	834.753141	15.942938
24.753242	840.281998	15.947955
24.612630	844.715711	15.952973
24.461667	839.469353	15.957991
24.978376	852.107186	15.963008
24.608129	862.471276	15.968026
24.597364	858.234429	15.973043
24.669169	867.031356	15.978061
24.341305	872.838394	15.983079
24.718480	865.117686	15.988096
24.433829	874.679692	15.993114
24.799606	875.295077	15.998131
25.138627	891.086935	16.003149
25.007375	884.528781	16.008167
24.818507	884.233052	16.013184
25.065082	889.991224	16.018202
25.245734	881.739306	16.023219
25.525446	885.146559	16.028237
25.474831	893.752057	16.033255
25.502821	889.816615	16.038272
25.371341	889.184985	16.043290
25.424825	881.875962	16.048307
25.442144	885.972129	16.053325
25.406426	886.044327	16.058343
25.695521	885.285333	16.063360
25.458703	886.335769	16.068378
25.580147	879.421742	16.073395
24.917571	882.075722	16.078413
25.491259	885.750480	16.083431
25.835135	883.023437	16.088448
25.557026	897.824668	16.093466
25.668201	886.849289	16.098483
25.271392	896.939791	16.103501
25.584057	887.266110	16.108519
25.780813	882.530972	16.113536
25.697697	884.709441	16.118554
26.012630	873.355483	16.123571
25.681305	878.021964	16.128589
25.665810	890.363595	16.133607
25.956244	879.918437	16.138624
25.433150	887.855689	16.143642
25.796659	887.125335	16.148659
25.981417	880.629606	16.153677
25.929174	883.566122	16.158695
25.660840	883.717206	16.163712
25.433217	895.241786	16.168730
25.843846	892.347440	16.173747
26.047223	912.195160	16.178765
25.878947	911.644006	16.183783
26.266227	913.182247	16.188800
26.161862	914.217292	16.193818
26.445181	903.228412	16.198835
26.266037	917.069284	16.203853
25.960265	910.774661	16.208871
26.215103	905.450396	16.213888
26.054948	912.214892	16.218906
26.328217	909.753404	16.223923
26.265505	904.784612	16.228941
26.120333	911.818236	16.233959
26.308199	900.933108	16.238976
26.429241	917.918583	16.243994
26.454406	900.875820	16.249011
26.650912	909.282054	16.254029
26.245475	903.728379	16.259047
26.456813	903.858257	16.264064
26.179600	911.399342	16.269082
26.352647	908.290264	16.274099
26.628405	912.746611	16.279117
26.581844	915.528481	16.284135
26.607253	912.472338	16.289152
26.592116	908.798796	16.294170
26.682283	907.162108	16.299187
26.698340	902.643504	16.304205
26.410021	906.752199	16.309223
26.719530	901.862423	16.314240
26.729846	911.306430	16.319258
26.710340	912.815651	16.324275
26.760521	890.731482	16.329293
26.690839	907.488667	16.334311
26.660083	909.453799	16.339328
26.430018	909.204043	16.344346
26.369013	899.735484	16.349363
26.951544	914.742773	16.354381
26.720825	926.012028	16.359399
27.081628	932.097045	16.364416
27.049051	949.263129	16.369434
26.928263	937.535241	16.374451
26.947305	932.482077	16.379469
26.822995	933.587434	16.384487
27.274293	933.681496	16.389504
27.257341	938.340426	16.394522
27.304381	932.339791	16.399539
27.015666	931.145074	16.404557
27.021023	937.095263	16.409575
27.483447	925.278782	16.414592
27.169776	934.936747	16.419610
27.217016	928.473761	16.424627
27.239105	934.595268	16.429645
27.336623	940.646251	16.434663
27.265937	934.039295	16.439680
27.220709	939.269333	16.444698
27.309100	934.582199	16.449715
27.010163	934.198181	16.454733
27.036783	938.400778	16.459751
27.503280	952.156441	16.464768
27.791636	958.104844	16.469786
27.425005	952.293603	16.474803
27.549044	957.561510	16.479821
27.590139	958.813914	16.484839
27.759513	964.941797	16.489856
27.644238	972.934807	16.494874
27.548211	970.907697	16.499891
27.691178	968.711981	16.504909
27.860188	967.256122	16.509927
27.954572	972.792275	16.514944
27.803036	969.047377	16.519962
27.973309	965.837287	16.524979
27.645068	956.095096	16.529997
27.654357	968.850042	16.535015
27.924618	961.219185	16.540032
28.005238	964.637215	16.545050
27.669000	969.084692	16.550067
27.960643	959.366122	16.555085
27.485356	956.752687	16.560103
27.838979	960.159651	16.565120
27.725399	959.362982	16.570138
27.630407	968.846764	16.575155
27.933357	969.751719	16.580173
28.234569	986.530559	16.585191
28.250289	985.234258	16.590208
28.317226	992.636046	16.595226
28.664127	983.738991	16.600243
28.705905	977.575457	16.605261
28.049440	969.039460	16.610279
28.223283	962.015771	16.615296
28.065958	967.999646	16.620314
27.955777	978.962162	16.625331
28.520972	985.150310	16.630349
28.373936	999.949857	16.635367
28.362199	994.155234	16.640384
28.478774	988.399439	16.645402
28.510795	985.375451	16.650419
28.768313	992.269056	16.655437
28.527294	988.672480	16.660455
28.412173	986.380557	16.665472
28.342190	987.163807	16.670490
28.315564	992.442649	16.675507
28.587824	984.974611	16.680525
28.556900	988.948486	16.685543
28.777195	984.444130	16.690560
28.682190	985.970460	16.695578
28.475169	998.019376	16.700595
29.218015	1012.287203	16.705613
28.905997	1019.913016	16.710631
29.363938	1003.571127	16.715648
29.357857	996.383685	16.720666
28.822387	986.368194	16.725683
29.084199	992.339892	16.730701
28.803040	987.028498	16.735719
29.242900	988.191095	16.740736
29.088659	985.193262	16.745754
28.838880	990.401912	16.750771
29.259915	989.140386	16.755789
28.938323	987.664337	16.760807
29.035982	991.747354	16.765824
29.046631	997.975581	16.770842
28.973579	1024.144316	16.775859
29.560778	1015.024790	16.780877
29.204787	1023.555846	16.785895
29.512327	1015.116775	16.790912
29.184583	1019.132425	16.795930
29.298492	1018.534340	16.800947
29.408663	1011.317740	16.805965
29.262531	1027.299735	16.810983
29.385335	1020.721288	16.816000
29.563268	1023.615168	16.821018
29.356022	1013.830213	16.826035
29.453573	1014.886022	16.831053
29.221507	1021.969483	16.836071
29.489365	1024.045295	16.841088
29.847226	1018.484713	16.846106
29.549230	1024.167207	16.851123
29.435497	1017.857633	16.856141
29.580326	1031.028247	16.861159
29.713343	1043.114987	16.866176
29.994522	1045.904522	16.871194
30.234015	1046.452707	16.876211
30.113236	1036.461257	16.881229
29.663782	1026.124394	16.886247
29.470857	1020.960583	16.891264
30.033779	1041.927594	16.896282
29.601554	1039.143276	16.901299
30.129725	1042.415527	16.906317
29.989590	1048.989602	16.911335
29.935623	1040.978501	16.916352
30.177145	1049.140405	16.921370
29.672240	1048.005022	16.926387
30.191681	1052.699538	16.931405
30.055791	1042.951682	16.936423
29.792915	1048.540306	16.941440
30.071930	1045.039147	16.946458
29.683088	1054.209595	16.951475
30.020151	1041.239434	16.956493
30.288880	1073.901147	16.961511
30.419876	1077.883419	16.966528
30.711792	1068.712772	16.971546
30.565830	1078.693546	16.976563
30.582633	1072.405284	16.981581
30.598347	1072.874328	16.986599
30.261861	1061.738392	16.991616
30.487725	1055.340208	16.996634
30.784565	1069.975148	17.001651
30.769063	1069.246996	17.006669
30.685231	1072.666443	17.011687
30.830163	1076.270490	17.016704
30.753613	1047.440662	17.021722
30.448469	1052.146857	17.026739
30.803793	1057.930126	17.031757
30.931146	1071.420834	17.036775
30.954869	1072.197164	17.041792
31.193466	1067.882542	17.046810
30.557833	1066.052740	17.051827
31.008775	1061.917167	17.056845
30.885103	1083.267136	17.061863
31.162500	1072.648147	17.066880
30.944538	1082.924435	17.071898
30.740828	1077.190437	17.076915
31.064364	1069.724709	17.081933
31.175710	1068.066497	17.086951
31.125758	1065.296746	17.091968
31.258074	1069.353982	17.096986
31.167315	1075.451484	17.102003
31.461976	1079.671823	17.107021
31.264223	1067.783749	17.112039
31.029965	1073.718381	17.117056
31.398615	1072.553974	17.122074
31.173639	1070.485670	17.127091
31.285245	1079.600201	17.132109
31.103552	1072.411236	17.137127
31.305756	1060.546626	17.142144
31.450566	1071.835807	17.147162
31.173944	1069.694358	17.152179
31.336684	1074.872361	17.157197
31.241588	1069.994679	17.162215
30.966249	1081.223989	17.167232
31.616698	1081.246271	17.172250
31.644791	1095.180692	17.177267
31.856898	1096.070160	17.182285
31.535456	1089.734261	17.187303
31.634770	1089.556920	17.192320
32.028153	1083.941338	17.197338
31.695539	1086.554995	17.202355
31.793049	1095.811409	17.207373
31.651832	1089.029261	17.212391
31.779994	1088.213598	17.217408
32.006086	1080.515781	17.222426
31.680885	1092.636064	17.227443
31.858080	1085.325986	17.232461
31.735236	1089.309861	17.237479
31.629014	1097.779214	17.242496
31.828266	1110.168493	17.247514
31.692070	1118.430838	17.252531
32.023635	1122.569709	17.257549
32.196850	1120.014406	17.262567
32.159357	1126.123989	17.267584
32.500242	1114.069715	17.272602
32.144730	1116.440942	17.277619
32.181839	1112.567804	17.282637
32.177377	1115.370505	17.287655
32.102269	1113.707279	17.292672
32.458892	1102.691776	17.297690
32.047855	1116.929257	17.302707
32.199478	1111.675217	17.307725
32.398472	1120.628899	17.312743
32.729838	1137.832574	17.317760
32.827243	1130.659262	17.322778
32.702576	1134.851092	17.327795
33.017573	1123.419295	17.332813
32.751599	1112.318316	17.337831
32.408435	1098.374082	17.342848
32.591077	1108.015974	17.347866
32.730868	1132.173377	17.352883
33.024361	1136.891480	17.357901
32.712491	1135.033163	17.362919
32.657719	1143.394646	17.367936
32.970217	1133.833616	17.372954
32.891506	1140.340305	17.377971
32.810414	1144.391692	17.382989
32.858555	1138.479854	17.388007
33.088809	1137.240101	17.393024
32.927190	1134.887151	17.398042
32.762007	1140.646050	17.403059
33.152011	1130.900982	17.408077
33.269019	1129.281388	17.413095
32.893895	1129.939803	17.418112
33.384686	1137.538799	17.423130
33.208866	1128.147822	17.428147
32.924642	1130.502154	17.433165
33.326546	1129.845549	17.438183
33.171421	1136.318022	17.443200
33.251103	1146.745526	17.448218
33.523736	1158.025063	17.453235
33.629938	1160.654195	17.458253
34.002888	1161.756616	17.463271
33.319286	1149.320521	17.468288
33.734722	1134.703150	17.473306
33.675258	1138.208924	17.478323
33.324866	1124.684296	17.483341
33.628372	1144.222315	17.488359
33.625993	1161.894880	17.493376
33.748864	1157.454303	17.498394
33.912064	1168.478157	17.503411
33.789203	1181.259841	17.508429
33.895727	1165.056353	17.513447
33.908976	1168.461746	17.518464
33.918441	1152.076705	17.523482
34.142493	1160.873736	17.528499
34.007196	1152.934865	17.533517
34.134640	1166.130807	17.538535
34.033149	1161.847166	17.543552
34.202862	1149.127171	17.548570
34.142955	1161.120413	17.553587
34.166647	1158.592765	17.558605
34.094802	1164.108728	17.563623
34.057206	1166.385504	17.568640
34.092938	1166.672532	17.573658
33.756195	1161.020516	17.578675
33.714650	1164.176738	17.583693
33.746644	1159.918276	17.588711
34.008299	1165.819016	17.593728
34.316076	1170.114366	17.598746
34.386718	1183.870802	17.603763
34.414002	1187.547064	17.608781
34.652393	1182.275710	17.613799
35.012490	1194.560734	17.618816
34.887222	1171.106758	17.623834
34.560147	1167.074335	17.628851
34.108968	1156.462319	17.633869
34.370281	1163.998478	17.638887
34.208984	1177.426760	17.643904
35.155255	1180.864952	17.648922
34.635367	1189.806389	17.653939
34.451974	1179.445530	17.658957
34.878520	1178.627003	17.663975
34.674042	1188.247498	17.668992
34.651013	1183.607633	17.674010
34.986454	1182.839983	17.679027
34.726367	1183.554378	17.684045
34.950585	1175.989085	17.689063
34.642356	1192.856069	17.694080
35.032920	1200.614155	17.699098
35.036628	1207.148978	17.704115
35.186963	1215.176063	17.709133
35.519642	1213.011847	17.714151
35.378382	1215.542337	17.719168
35.674363	1202.777223	17.724186
35.451540	1197.758822	17.729203
35.243521	1180.519085	17.734221
35.351089	1177.729779	17.739239
35.038080	1190.830838	17.744256
35.415272	1199.389036	17.749274
35.554335	1211.095148	17.754291
35.572454	1210.950708	17.759309
35.986425	1207.973384	17.764327
35.813728	1210.276034	17.769344
35.535876	1195.471646	17.774362
35.503727	1198.269490	17.779379
35.541317	1206.430144	17.784397
35.792134	1205.784923	17.789415
35.262557	1205.475323	17.794432
35.509576	1209.466602	17.799450
35.647876	1205.260234	17.804467
35.245436	1209.331281	17.809485
35.458239	1198.803575	17.814503
35.801710	1224.636442	17.819520
35.663097	1232.886848	17.824538
36.091936	1238.011290	17.829555
36.018076	1238.920468	17.834573
36.200654	1228.086172	17.839591
36.045939	1243.025191	17.844608
36.214807	1231.746378	17.849626
36.089455	1231.709886	17.854643
35.994335	1234.042037	17.859661
36.190205	1234.335669	17.864679
36.339343	1240.827776	17.869696
36.489729	1229.475457	17.874714
36.787485	1231.094362	17.879731
36.370590	1241.749440	17.884749
36.647677	1234.803433	17.889767
36.612957	1241.814822	17.894784
36.727325	1225.533411	17.899802
36.481993	1237.387696	17.904819
36.612997	1243.598397	17.909837
36.483514	1232.590112	17.914855
36.373030	1234.751601	17.919872
36.536258	1231.859795	17.924890
36.330456	1230.721419	17.929907
36.235378	1229.161858	17.934925
36.786293	1235.172084	17.939943
36.289364	1238.832246	17.944960
36.614382	1255.936528	17.949978
37.024597	1271.415585	17.954995
37.126814	1265.249525	17.960013
37.332938	1258.462258	17.965031
37.130071	1256.863822	17.970048
36.988102	1260.625740	17.975066
37.105791	1263.880256	17.980083
37.011462	1268.044474	17.985101
37.343128	1256.093567	17.990119
37.368163	1262.381423	17.995136
37.221480	1257.172890	18.000154
36.987959	1261.978909	18.005171
36.937045	1258.909132	18.010189
37.465415	1258.722886	18.015207
37.039310	1268.652650	18.020224
37.314396	1256.125160	18.025242
37.309165	1263.602479	18.030259
36.983791	1257.625173	18.035277
37.234499	1249.969064	18.040295
37.411911	1264.033073	18.045312
37.509777	1276.265449	18.050330
37.760960	1281.450557	18.055347
37.644116	1284.312011	18.060365
38.197888	1273.080175	18.065383
38.365270	1275.222913	18.070400
37.892990	1264.819985	18.075418
37.756752	1260.695775	18.080435
37.955506	1252.792777	18.085453
37.797079	1260.433774	18.090471
37.818057	1258.031341	18.095488
38.277833	1274.356605	18.100506
38.207105	1279.292987	18.105523
38.193196	1259.240218	18.110541
38.222742	1265.392116	18.115559
38.100388	1253.471953	18.120576
37.920478	1255.692941	18.125594
37.891201	1260.519531	18.130611
38.184031	1274.711107	18.135629
38.235069	1269.995601	18.140647
38.222733	1279.941827	18.145664
38.186661	1275.281652	18.150682
38.112935	1283.803996	18.155699
38.036760	1284.549805	18.160717
38.028045	1276.886560	18.165735
38.459798	1284.464288	18.170752
38.361279	1295.295102	18.175770
38.791226	1302.100421	18.180787
39.008503	1304.422488	18.185805
38.791242	1295.755076	18.190823
38.477309	1288.391436	18.195840
38.688039	1290.740760	18.200858
39.156594	1294.087475	18.205875
38.738530	1313.364693	18.210893
38.830114	1304.966466	18.215911
39.078416	1306.382757	18.220928
39.079635	1304.565186	18.225946
39.162196	1299.148703	18.230963
39.167212	1312.157751	18.235981
38.952993	1290.746130	18.240999
39.453709	1293.223885	18.246016
38.997116	1279.947144	18.251034
39.266372	1280.244987	18.256051
38.899627	1285.418250	18.261069
38.935476	1293.187764	18.266087
39.114988	1303.115685	18.271104
38.882211	1307.268546	18.276122
39.295229	1299.366333	18.281139
38.996955	1300.977457	18.286157
39.319081	1311.144374	18.291175
39.216315	1303.204773	18.296192
39.574413	1298.910491	18.301210
39.193614	1309.582088	18.306227
39.194584	1310.695211	18.311245
39.151018	1328.395833	18.316263
39.282277	1332.787318	18.321280
39.536790	1331.495320	18.326298
39.731040	1326.432165	18.331315
39.374006	1333.002839	18.336333
39.753228	1333.394895	18.341351
39.709903	1322.973199	18.346368
40.059584	1352.331096	18.351386
40.639535	1338.455127	18.356403
40.211015	1314.385005	18.361421
40.284684	1318.932436	18.366439
40.405245	1323.101901	18.371456
40.024080	1317.895486	18.376474
40.517015	1309.673415	18.381491
40.661474	1310.817148	18.386509
40.566346	1316.029382	18.391527
40.717505	1313.881765	18.396544
40.144091	1314.561735	18.401562
40.314534	1308.082068	18.406579
40.295428	1305.632324	18.411597
40.139134	1304.932149	18.416615
40.371671	1307.426865	18.421632
40.235659	1318.111552	18.426650
40.417766	1300.339764	18.431667
40.569295	1315.178845	18.436685
40.562664	1299.411960	18.441703
40.846590	1304.766442	18.446720
40.579037	1300.986114	18.451738
40.905269	1304.936773	18.456755
40.901710	1301.424190	18.461773
40.556885	1304.488257	18.466791
40.433110	1303.651824	18.471808
40.586730	1326.649749	18.476826
41.049413	1329.649267	18.481843
40.862111	1342.108516	18.486861
41.197314	1335.658492	18.491879
41.370236	1330.528398	18.496896
40.826784	1342.122232	18.501914
41.001740	1323.699926	18.506931
40.844775	1342.043225	18.511949
40.869869	1342.656965	18.516967
41.151169	1334.602117	18.521984
41.082591	1342.979767	18.527002
41.441655	1354.138293	18.532019
41.572128	1357.011443	18.537037
41.467653	1361.070686	18.542055
41.648447	1360.445298	18.547072
41.840779	1359.407631	18.552090
41.756037	1342.183556	18.557107
41.713073	1333.926032	18.562125
41.599979	1345.620774	18.567143
41.796483	1337.305766	18.572160
41.570534	1345.145729	18.577178
42.122787	1338.785604	18.582195
41.912016	1353.302170	18.587213
41.931071	1343.764505	18.592231
41.852710	1333.142521	18.597248
41.684561	1341.150266	18.602266
41.760506	1347.674196	18.607283
42.265893	1357.285349	18.612301
42.025556	1362.677871	18.617319
42.086751	1356.293981	18.622336
41.754482	1354.846426	18.627354
42.212267	1350.115641	18.632371
42.090659	1357.640382	18.637389
41.635493	1362.928661	18.642407
42.029137	1357.908125	18.647424
41.961976	1357.916141	18.652442
41.976322	1370.828436	18.657459
42.413883	1392.593889	18.662477
42.311756	1398.996896	18.667495
42.605311	1386.575090	18.672512
42.331235	1385.656025	18.677530
42.585788	1378.885108	18.682547
42.902878	1391.587573	18.687565
42.717798	1389.191616	18.692583
42.974465	1383.526483	18.697600
42.572400	1389.398428	18.702618
43.005978	1380.189623	18.707635
42.704247	1388.623934	18.712653
43.331761	1386.451518	18.717671
42.928359	1383.977090	18.722688
42.918665	1394.067419	18.727706
42.911449	1381.898439	18.732723
43.121811	1372.211248	18.737741
42.895049	1394.841685	18.742759
43.044429	1374.175453	18.747776
42.739788	1385.902862	18.752794
42.699723	1395.905902	18.757811
43.118435	1402.999892	18.762829
43.368376	1414.067258	18.767847
43.695771	1406.213190	18.772864
43.424439	1407.354390	18.777882
43.627415	1402.635583	18.782899
43.712789	1397.427034	18.787917
43.522233	1400.934061	18.792935
43.736753	1409.674748	18.797952
43.549317	1406.860736	18.802970
43.695011	1410.124039	18.807987
43.882685	1396.685622	18.813005
43.678288	1407.922537	18.818023
43.842183	1411.528451	18.823040
43.446446	1410.201599	18.828058
43.588444	1409.653475	18.833075
44.040492	1406.284248	18.838093
43.603309	1410.480952	18.843111
44.240621	1426.331634	18.848128
44.194845	1438.446755	18.853146
44.265977	1432.640831	18.858163
44.365690	1427.563348	18.863181
44.235548	1413.555676	18.868199
44.597580	1405.709858	18.873216
44.028767	1402.111356	18.878234
44.235120	1413.496903	18.883251
44.259241	1430.262184	18.888269
44.428516	1430.024861	18.893287
44.477993	1431.027431	18.898304
44.163773	1441.471220	18.903322
44.225980	1431.481750	18.908339
44.386245	1434.206311	18.913357
44.453080	1430.923960	18.918375
44.664983	1430.868541	18.923392
44.547923	1434.211484	18.928410
44.499720	1434.369692	18.933427
44.867089	1445.717632	18.938445
44.777656	1452.827713	18.943463
45.188586	1448.428610	18.948480
45.071766	1451.725855	18.953498
45.156353	1443.403697	18.958515
45.131073	1443.608110	18.963533
44.953403	1453.592397	18.968551
45.237671	1452.058893	18.973568
45.022975	1453.371420	18.978586
45.298736	1454.995953	18.983603
45.089310	1445.931155	18.988621
44.986811	1450.503407	18.993639
45.335877	1439.651291	18.998656
45.487598	1449.260521	19.003674
45.370225	1446.217239	19.008691
45.097886	1449.518926	19.013709
45.166784	1445.184414	19.018727
45.625428	1441.080535	19.023744
45.236558	1446.732832	19.028762
45.439555	1469.744266	19.033779
45.554295	1469.658256	19.038797
45.396235	1473.222519	19.043815
45.774837	1473.776077	19.048832
45.910294	1472.930256	19.053850
45.685757	1479.103363	19.058867
46.052129	1474.576989	19.063885
45.853397	1482.172007	19.068903
46.109099	1468.563648	19.073920
45.994698	1473.460268	19.078938
45.857887	1470.671928	19.083955
46.191099	1471.239875	19.088973
45.928215	1475.209200	19.093991
46.317879	1486.922923	19.099008
46.406313	1488.406983	19.104026
46.508225	1502.332527	19.109043
46.649696	1497.641765	19.114061
46.230074	1503.778035	19.119079
46.524110	1500.848424	19.124096
46.601500	1499.123149	19.129114
46.742706	1495.471655	19.134131
47.044794	1490.074332	19.139149
46.721824	1501.485612	19.144167
46.716703	1499.702525	19.149184
46.862514	1491.466274	19.154202
46.903684	1491.974622	19.159219
47.079374	1496.697740	19.164237
47.021528	1495.830522	19.169255
47.051588	1490.518106	19.174272
46.839827	1493.762948	19.179290
46.886379	1496.485055	19.184307
47.281880	1495.529735	19.189325
47.131224	1490.265093	19.194343
47.072858	1493.695974	19.199360
46.911559	1484.138229	19.204378
46.886648	1490.642277	19.209395
47.208988	1490.934699	19.214413
47.178251	1513.764578	19.219431
47.413235	1517.032044	19.224448
47.523938	1524.820403	19.229466
47.597272	1520.786473	19.234483
47.789501	1525.817650	19.239501
47.746937	1523.812434	19.244519
47.930359	1526.394031	19.249536
48.085286	1519.662151	19.254554
47.800621	1531.263945	19.259571
47.665956	1526.657186	19.264589
47.544589	1530.939314	19.269607
47.796046	1529.189996	19.274624
47.685317	1523.416059	19.279642
47.713272	1533.736642	19.284659
47.900023	1525.691415	19.289677
47.580540	1527.507810	19.294695
47.919841	1522.525330	19.299712
47.968740	1526.957445	19.304730
48.076097	1541.568447	19.309747
48.059492	1540.913082	19.314765
47.926450	1557.459429	19.319783
48.393436	1549.342687	19.324800
48.455198	1539.389435	19.329818
48.646174	1547.597945	19.334835
49.024635	1541.516030	19.339853
48.354296	1543.832273	19.344871
48.393168	1545.748486	19.349888
48.747312	1548.430007	19.354906
48.572007	1548.604889	19.359923
48.565830	1542.517252	19.364941
48.305850	1540.966014	19.369959
48.601089	1568.604033	19.374976
48.756613	1564.478568	19.379994
48.451752	1569.027807	19.385011
48.991353	1558.895791	19.390029
48.654369	1574.304758	19.395047
49.067181	1571.535009	19.400064
49.082542	1564.562428	19.405082
49.085377	1574.495118	19.410099
49.297853	1575.016691	19.415117
49.608439	1598.869280	19.420135
49.513840	1587.478648	19.425152
49.764643	1571.728778	19.430170
49.493306	1566.641117	19.435187
49.575734	1564.145030	19.440205
49.146986	1569.580173	19.445223
49.565841	1583.340440	19.450240
49.525323	1591.476023	19.455258
49.888521	1592.408261	19.460275
49.993677	1588.979799	19.465293
49.946618	1591.390270	19.470311
50.134399	1594.072129	19.475328
49.973279	1591.258654	19.480346
49.577278	1598.605263	19.485363
49.978750	1587.335778	19.490381
49.831582	1598.798776	19.495399
49.543372	1601.727381	19.500416
50.156504	1584.369210	19.505434
50.108383	1600.353809	19.510451
49.886961	1597.332020	19.515469
49.975128	1612.624319	19.520487
50.293476	1622.005559	19.525504
50.524443	1620.038583	19.530522
50.536657	1629.959917	19.535539
50.277969	1614.479605	19.540557
50.237309	1619.159192	19.545575
50.476906	1615.762437	19.550592
50.579603	1617.975354	19.555610
50.784068	1613.406020	19.560627
50.961636	1620.077227	19.565645
50.786286	1623.665245	19.570663
50.642016	1624.993901	19.575680
50.694533	1610.864341	19.580698
50.771479	1628.800479	19.585715
51.289901	1640.558585	19.590733
51.990831	1627.865161	19.595751
51.897215	1610.037804	19.600768
52.243865	1593.133840	19.605786
51.943459	1598.421425	19.610803
52.135336	1580.860268	19.615821
51.903874	1566.881205	19.620839
52.077713	1563.569728	19.625856
51.808091	1562.417860	19.630874
51.632079	1552.969969	19.635891
51.868552	1554.948202	19.640909
51.515105	1544.239067	19.645927
51.680030	1546.933946	19.650944
51.864115	1543.412541	19.655962
51.609796	1558.800943	19.660979
51.672582	1548.575506	19.665997
51.656695	1545.234960	19.671015
51.372463	1554.894056	19.676032
51.778610	1551.543996	19.681050
51.399177	1556.277381	19.686067
51.670965	1547.982885	19.691085
51.739031	1550.496947	19.696103
51.890905	1575.198448	19.701120
52.091597	1577.307186	19.706138
51.725279	1603.330415	19.711155
52.092031	1584.206311	19.716173
52.176631	1591.983075	19.721191
52.116681	1594.141381	19.726208
52.327758	1578.440779	19.731226
52.137430	1604.880734	19.736243
52.268177	1604.160077	19.741261
52.251810	1613.353939	19.746279
52.259020	1613.148512	19.751296
52.381709	1610.755985	19.756314
52.530099	1615.690907	19.761331
52.907542	1633.658289	19.766349
52.819589	1644.422454	19.771367
53.066528	1640.755619	19.776384
53.140160	1647.441651	19.781402
52.948882	1640.860223	19.786419
53.204305	1644.600850	19.791437
53.123243	1645.241986	19.796455
53.340682	1642.079960	19.801472
53.490685	1641.380722	19.806490
53.191550	1650.004682	19.811507
53.605907	1632.465750	19.816525
53.294834	1640.350240	19.821543
53.001526	1644.452965	19.826560
53.686520	1629.112523	19.831578
53.396100	1640.963743	19.836595
53.301751	1637.486359	19.841613
53.583753	1640.045387	19.846631
53.582990	1639.156722	19.851648
53.701753	1645.746331	19.856666
53.590016	1656.011548	19.861683
53.848656	1668.759330	19.866701
54.110938	1664.662648	19.871719
54.013922	1674.958314	19.876736
54.128066	1669.082604	19.881754
54.176740	1672.104155	19.886771
53.914155	1671.932878	19.891789
54.028692	1661.312645	19.896807
53.826975	1673.736950	19.901824
54.290045	1657.377384	19.906842
54.274933	1663.711601	19.911859
53.992776	1659.053201	19.916877
54.461940	1667.761404	19.921895
54.615969	1684.256709	19.926912
54.653608	1694.745070	19.931930
54.882762	1693.139164	19.936947
54.892253	1694.743559	19.941965
55.142872	1681.835368	19.946983
55.010847	1673.699846	19.952000
54.882351	1666.917898	19.957018
54.751151	1662.797076	19.962035
54.895373	1671.815834	19.967053
55.098105	1680.092739	19.972071
55.097015	1687.196989	19.977088
55.395200	1686.460076	19.982106
55.444710	1688.692618	19.987123
55.276296	1678.256120	19.992141
55.053010	1662.571508	19.997159
55.205237	1676.853417	20.002176
55.467980	1677.803638	20.007194
55.390075	1688.019590	20.012211
55.284087	1685.744161	20.017229
55.282068	1678.940915	20.022247
55.282344	1685.731397	20.027264
55.255004	1688.097685	20.032282
55.293595	1681.986259	20.037299
55.392517	1700.770708	20.042317
55.684226	1715.428961	20.047335
55.512462	1713.418104	20.052352
55.894391	1710.559155	20.057370
55.656707	1715.891723	20.062387
55.683380	1714.755046	20.067405
56.304811	1725.857695	20.072423
55.855401	1750.289199	20.077440
56.299586	1743.405498	20.082458
56.537625	1743.978162	20.087475
56.128216	1754.388094	20.092493
56.372340	1744.941122	20.097511
56.218777	1747.740234	20.102528
56.324534	1745.639425	20.107546
56.621686	1743.916779	20.112563
56.396588	1744.217987	20.117581
56.590767	1737.376192	20.122599
56.488378	1746.557580	20.127616
56.610223	1753.106770	20.132634
56.687284	1775.978273	20.137651
56.859696	1778.503866	20.142669
57.031534	1763.234311	20.147687
56.820482	1780.382297	20.152704
57.209783	1771.942295	20.157722
56.880097	1775.152751	20.162739
57.137363	1766.378118	20.167757
57.532564	1760.486437	20.172775
57.453797	1773.922268	20.177792
57.722277	1768.419983	20.182810
57.360690	1762.369142	20.187827
57.766488	1765.948944	20.192845
57.727415	1766.787058	20.197863
57.314126	1765.839995	20.202880
57.579746	1762.756782	20.207898
57.501439	1762.731409	20.212915
57.633801	1773.608845	20.217933
57.880625	1776.508314	20.222951
57.975204	1798.366056	20.227968
58.135308	1796.090138	20.232986
57.963152	1809.027714	20.238003
57.715813	1791.331246	20.243021
58.207740	1795.243236	20.248039
58.233938	1798.495861	20.253056
58.211324	1794.338362	20.258074
58.148010	1795.847724	20.263091
58.122900	1796.269410	20.268109
57.945947	1794.458589	20.273127
58.056334	1790.131296	20.278144
58.560277	1796.418570	20.283162
58.579247	1804.081695	20.288179
58.430870	1812.261789	20.293197
58.944012	1804.772840	20.298215
58.740977	1808.815028	20.303232
58.821637	1809.004694	20.308250
58.539543	1804.876096	20.313267
58.758123	1812.599536	20.318285
58.791506	1794.915330	20.323303
58.705500	1804.001733	20.328320
59.370444	1799.768209	20.333338
59.307494	1793.226131	20.338355
58.939999	1799.153140	20.343373
59.345354	1792.082551	20.348391
59.094798	1800.476940	20.353408
59.168753	1810.028980	20.358426
59.521635	1818.325040	20.363443
59.765293	1825.388320	20.368461
59.815120	1822.037248	20.373479
59.478209	1826.614493	20.378496
59.983822	1819.848348	20.383514
60.161351	1822.763410	20.388531
59.964354	1824.515116	20.393549
60.225534	1809.975150	20.398567
60.087399	1803.751754	20.403584
59.740486	1787.584749	20.408602
59.903001	1800.643765	20.413619
60.190440	1813.167448	20.418637
60.249268	1818.675632	20.423655
59.967014	1821.966242	20.428672
60.119141	1815.984211	20.433690
60.316468	1810.600546	20.438707
60.082174	1808.393735	20.443725
60.384283	1811.775552	20.448743
60.502430	1813.721409	20.453760
60.295949	1813.886486	20.458778
60.319530	1819.510128	20.463795
60.345474	1838.466234	20.468813
60.752187	1829.183266	20.473831
60.890076	1845.412546	20.478848
60.883316	1844.196749	20.483866
60.809722	1834.954765	20.488883
60.909200	1835.031887	20.493901
61.243131	1835.991219	20.498919
61.114546	1842.898329	20.503936
61.142908	1834.417358	20.508954
61.276977	1837.607288	20.513971
61.137736	1842.951188	20.518989
61.072673	1848.702664	20.524007
61.475746	1861.691275	20.529024
61.241247	1878.299805	20.534042
61.660224	1867.191772	20.539059
61.733956	1866.391952	20.544077
61.776300	1868.477887	20.549095
61.661344	1862.392550	20.554112
62.087171	1863.243205	20.559130
62.059881	1848.939235	20.564147
62.155318	1861.682655	20.569165
62.258757	1857.674367	20.574183
62.061581	1873.095761	20.579200
62.201852	1858.594625	20.584218
62.366141	1861.629191	20.589235
62.286839	1861.513048	20.594253
62.576415	1850.383895	20.599271
62.354617	1864.818718	20.604288
62.121920	1872.952155	20.609306
62.519443	1861.166649	20.614323
62.054680	1862.088890	20.619341
62.590453	1865.957241	20.624359
62.913271	1877.056988	20.629376
62.587495	1883.262141	20.634394
63.164516	1886.542253	20.639411
62.807355	1880.149138	20.644429
63.167764	1878.328633	20.649447
63.045351	1879.871389	20.654464
63.198495	1875.383876	20.659482
63.744630	1878.714557	20.664499
63.019594	1873.354562	20.669517
63.175828	1877.266738	20.674535
63.196798	1878.550395	20.679552
63.257383	1868.792968	20.684570
63.654304	1867.178415	20.689587
63.641620	1867.278598	20.694605
63.410518	1870.281074	20.699623
63.359874	1863.120863	20.704640
63.192034	1878.286460	20.709658
63.612432	1876.520209	20.714675
63.357810	1881.812330	20.719693
63.686430	1895.132331	20.724711
63.740311	1904.148438	20.729728
63.944155	1907.884467	20.734746
63.967036	1895.901227	20.739763
63.791476	1905.372328	20.744781
63.957736	1896.489445	20.749799
64.124789	1901.880968	20.754816
64.215775	1896.479810	20.759834
64.384758	1897.351456	20.764851
64.571001	1921.693348	20.769869
64.601403	1912.993911	20.774887
64.392663	1916.256647	20.779904
64.463850	1922.186596	20.784922
65.187387	1918.559037	20.789939
64.366281	1917.866340	20.794957
64.952100	1914.206230	20.799975
64.789817	1912.654161	20.804992
64.940357	1922.006039	20.810010
64.959960	1910.522091	20.815027
65.121242	1917.638588	20.820045
65.401856	1928.551472	20.825063
65.077768	1921.182905	20.830080
64.734167	1918.330043	20.835098
65.159366	1933.705733	20.840115
65.417612	1948.034736	20.845133
65.436405	1942.087484	20.850151
65.753391	1957.723571	20.855168
65.485233	1955.918748	20.860186
65.898621	1932.392313	20.865203
65.792391	1939.088314	20.870221
65.654849	1949.349527	20.875239
65.543620	1945.431801	20.880256
65.317678	1955.928664	20.885274
65.905048	1957.742088	20.890291
65.768366	1969.414038	20.895309
66.147749	1976.031581	20.900327
66.126999	1973.834729	20.905344
66.090774	1989.340457	20.910362
66.516494	1971.702029	20.915379
66.170599	1971.044767	20.920397
66.083398	1982.096413	20.925415
66.680544	1990.003422	20.930432
66.676434	2004.557308	20.935450
66.821288	2005.612850	20.940467
66.687727	2006.651610	20.945485
66.846085	1994.108169	20.950503
66.817929	2002.175594	20.955520
66.907617	2007.678156	20.960538
66.910945	1995.485100	20.965555
67.257337	1998.321904	20.970573
67.400011	2008.746277	20.975591
67.423300	1997.581700	20.980608
67.266971	1996.897244	20.985626
67.603325	1992.128465	20.990643
67.316567	1991.854890	20.995661
67.466865	1995.833031	21.000679
67.719308	1994.069524	21.005696
67.746121	1998.626278	21.010714
67.366575	1992.309838	21.015731
67.311618	1988.809528	21.020749
67.586008	2006.606208	21.025767
68.009278	2010.874249	21.030784
67.681770	2014.582175	21.035802
68.176233	2017.886194	21.040819
68.075382	2019.142753	21.045837
68.170192	2015.929270	21.050855
68.188299	2014.531023	21.055872
67.777889	2019.075789	21.060890
68.275792	2005.839291	21.065907
68.117081	2021.207434	21.070925
68.222678	2017.445376	21.075943
68.566397	2029.283236	21.080960
68.348967	2037.726998	21.085978
68.828916	2053.290786	21.090995
68.756873	2051.903693	21.096013
68.691455	2037.767052	21.101031
68.948951	2045.104299	21.106048
68.522337	2046.275730	21.111066
69.393930	2034.385379	21.116083
68.875221	2042.342962	21.121101
69.064910	2043.759956	21.126119
69.026916	2041.203778	21.131136
69.398656	2056.062102	21.136154
69.447568	2050.751102	21.141171
69.644540	2069.056265	21.146189
69.477667	2067.910211	21.151207
69.822907	2060.215642	21.156224
69.600244	2063.981443	21.161242
69.970983	2047.010411	21.166259
69.807889	2058.008124	21.171277
69.771859	2070.186298	21.176295
69.924375	2062.668835	21.181312
69.798179	2061.957352	21.186330
69.626002	2061.827816	21.191347
70.021541	2060.891157	21.196365
69.625654	2090.335876	21.201383
70.462573	2078.016621	21.206400
70.285811	2094.724099	21.211418
70.568372	2085.626831	21.216435
70.666737	2085.166004	21.221453
70.524380	2084.689254	21.226471
70.592697	2080.770956	21.231488
70.606634	2085.052332	21.236506
70.994874	2086.404044	21.241523
70.947813	2087.532441	21.246541
70.853998	2078.286764	21.251559
71.247694	2077.434455	21.256576
70.696925	2092.316330	21.261594
71.205646	2097.004088	21.266611
71.494868	2114.516582	21.271629
71.219410	2114.661961	21.276647
71.531007	2112.472763	21.281664
71.369162	2104.822205	21.286682
71.842830	2111.247080	21.291699
71.977054	2106.876788	21.296717
71.511340	2109.838361	21.301735
71.898801	2102.002556	21.306752
71.863569	2115.683237	21.311770
72.194458	2104.209117	21.316787
71.890361	2105.942925	21.321805
71.687982	2111.201100	21.326823
71.949659	2095.455591	21.331840
71.589316	2113.640718	21.336858
71.834803	2111.576606	21.341875
72.121130	2108.743422	21.346893
72.107997	2129.948637	21.351911
72.292280	2133.498799	21.356928
72.170873	2144.995146	21.361946
72.491389	2129.453442	21.366963
72.453940	2143.462433	21.371981
72.255529	2138.399731	21.376999
72.636988	2125.777983	21.382016
72.705337	2141.597849	21.387034
73.038041	2151.470891	21.392051
72.683544	2152.338906	21.397069
73.218418	2151.555972	21.402087
73.470837	2141.703884	21.407104
73.284386	2149.792032	21.412122
73.412239	2142.471107	21.417139
73.346881	2141.962931	21.422157
73.312238	2147.410506	21.427175
73.603158	2140.814529	21.432192
73.252267	2141.322337	21.437210
73.584190	2144.560732	21.442227
73.707605	2141.730646	21.447245
73.218547	2155.643228	21.452263
73.611416	2162.913088	21.457280
73.710838	2177.128209	21.462298
73.743844	2174.219759	21.467315
74.139718	2171.993007	21.472333
73.744856	2179.445990	21.477351
74.180311	2181.710685	21.482368
74.088974	2201.576296	21.487386
74.520185	2196.868544	21.492403
74.637612	2201.355665	21.497421
74.291037	2206.171997	21.502439
74.392986	2197.890654	21.507456
74.465501	2207.878373	21.512474
74.191183	2195.440122	21.517491
74.446500	2212.632180	21.522509
74.790256	2222.838646	21.527527
75.116345	2224.869081	21.532544
75.426926	2216.411140	21.537562
75.775567	2227.195487	21.542579
75.260089	2215.709582	21.547597
75.641515	2215.912935	21.552615
75.908885	2205.592041	21.557632
76.108170	2208.598062	21.562650
75.794557	2210.696017	21.567667
75.902870	2191.656581	21.572685
75.616029	2183.988454	21.577703
75.818956	2202.058562	21.582720
75.885515	2201.445720	21.587738
75.975746	2203.100796	21.592755
76.228020	2203.368596	21.597773
76.353529	2212.366553	21.602791
76.571750	2210.137462	21.607808
76.407857	2207.975646	21.612826
76.167696	2212.072297	21.617843
76.372952	2209.222573	21.622861
75.823339	2207.647477	21.627879
76.187099	2196.962664	21.632896
76.391244	2212.071450	21.637914
76.303104	2197.571522	21.642931
76.452726	2217.584720	21.647949
76.547106	2225.719801	21.652967
76.515664	2226.636199	21.657984
76.666528	2227.056964	21.663002
76.673156	2238.105886	21.668019
77.022840	2232.794133	21.673037
77.076602	2254.762606	21.678055
77.240015	2253.402525	21.683072
77.474071	2259.893827	21.688090
77.544614	2259.787758	21.693107
77.709332	2257.089199	21.698125
77.457838	2260.642115	21.703143
77.551121	2253.365822	21.708160
77.683279	2263.301600	21.713178
77.591451	2267.632195	21.718195
78.061376	2250.554794	21.723213
77.433647	2259.944152	21.728231
77.636482	2270.656962	21.733248
77.922092	2276.105988	21.738266
77.749966	2283.065563	21.743283
78.124159	2286.577490	21.748301
77.950891	2292.075776	21.753319
78.361395	2283.015316	21.758336
78.201474	2295.098402	21.763354
78.211130	2310.176042	21.768371
78.846691	2316.748055	21.773389
79.258037	2313.754424	21.778407
79.459075	2304.216405	21.783424
79.360094	2306.460780	21.788442
79.173760	2306.064708	21.793459
79.574869	2291.934593	21.798477
79.252498	2284.476992	21.803495
79.633497	2268.426183	21.808512
79.255770	2268.406785	21.813530
79.161636	2267.614411	21.818547
79.440472	2285.404972	21.823565
79.406046	2296.747111	21.828583
79.371499	2305.878255	21.833600
79.546488	2304.055274	21.838618
79.368044	2303.990939	21.843635
79.511575	2299.089968	21.848653
79.597026	2318.522222	21.853671
79.722364	2315.177658	21.858688
79.822375	2330.261842	21.863706
79.912607	2323.301544	21.868723
80.187636	2320.693595	21.873741
80.080687	2332.934477	21.878759
80.524401	2349.197998	21.883776
81.041256	2347.032719	21.888794
80.925193	2335.264600	21.893811
81.056400	2346.006424	21.898829
81.255365	2339.931420	21.903847
81.001546	2322.266509	21.908864
80.831280	2312.522148	21.913882
80.722226	2321.568377	21.918899
81.227024	2331.289880	21.923917
81.015104	2339.818125	21.928935
81.188895	2342.205998	21.933952
80.980878	2340.832096	21.938970
81.127790	2349.958672	21.943987
81.490965	2338.260756	21.949005
81.220597	2351.574827	21.954023
81.325098	2365.441872	21.959040
81.597240	2369.284829	21.964058
81.455504	2369.767333	21.969075
81.808970	2374.217863	21.974093
81.691827	2370.467922	21.979111
81.866518	2378.035331	21.984128
82.200795	2388.903261	21.989146
81.943798	2408.283760	21.994163
82.476429	2400.572623	21.999181
82.051174	2401.708228	22.004199
82.340194	2402.800403	22.009216
82.512140	2403.518255	22.014234
82.537576	2400.273246	22.019251
82.640201	2395.122332	22.024269
82.554401	2405.635708	22.029287
82.993845	2398.219476	22.034304
83.021683	2397.078424	22.039322
82.739320	2419.785884	22.044339
83.104692	2414.818891	22.049357
83.067812	2434.982274	22.054375
82.956991	2416.706272	22.059392
83.442814	2421.997079	22.064410
83.056927	2419.808536	22.069427
83.339201	2422.507602	22.074445
83.352705	2425.850639	22.079463
83.351809	2432.982364	22.084480
83.755542	2447.604106	22.089498
83.417236	2458.213569	22.094515
83.975898	2446.651760	22.099533
83.779291	2447.292141	22.104551
83.985449	2451.865649	22.109568
83.855021	2449.412072	22.114586
84.180541	2457.277800	22.119603
84.125909	2467.638048	22.124621
83.950726	2469.966096	22.129639
84.219785	2476.095040	22.134656
84.761808	2471.396059	22.139674
84.315258	2488.833135	22.144691
84.697334	2507.070242	22.149709
84.999329	2506.539932	22.154727
85.012556	2508.708712	22.159744
85.232031	2505.395005	22.164762
85.132878	2512.519974	22.169779
85.380055	2499.945503	22.174797
85.464836	2510.345139	22.179815
85.421052	2507.619381	22.184832
85.666888	2495.321689	22.189850
85.425155	2507.046047	22.194867
85.473667	2501.550129	22.199885
85.618050	2502.067045	22.204903
85.484079	2505.778143	22.209920
85.530595	2515.273152	22.214938
85.641869	2516.968482	22.219955
85.874785	2520.097147	22.224973
85.876451	2529.570050	22.229991
85.788635	2549.836875	22.235008
86.692388	2540.254241	22.240026
86.706907	2547.486417	22.245043
87.221764	2545.024810	22.250061
86.990437	2539.703655	22.255079
86.579078	2547.214456	22.260096
87.089262	2537.312044	22.265114
86.815695	2540.617902	22.270131
86.970436	2546.188642	22.275149
87.048747	2534.956124	22.280167
87.252754	2542.315832	22.285184
87.256373	2538.138247	22.290202
87.046800	2541.664223	22.295219
87.224828	2536.205746	22.300237
87.231223	2531.810594	22.305255
87.359255	2549.923996	22.310272
88.011293	2551.849635	22.315290
87.458140	2569.783122	22.320307
87.976152	2566.375390	22.325325
87.697486	2566.713019	22.330343
87.414797	2568.360471	22.335360
87.483203	2568.467730	22.340378
87.374178	2584.165599	22.345395
87.878098	2595.247555	22.350413
88.052353	2594.709218	22.355431
88.195084	2591.829405	22.360448
88.607763	2597.700430	22.365466
88.341129	2596.084437	22.370483
88.426730	2614.020489	22.375501
88.630500	2623.816919	22.380519
89.191607	2624.533071	22.385536
89.289454	2613.703342	22.390554
89.258929	2611.471009	22.395571
89.451207	2624.478763	22.400589
89.448394	2616.004088	22.405607
89.457537	2607.765419	22.410624
89.607008	2612.706192	22.415642
89.593142	2610.128020	22.420659
89.312231	2600.778308	22.425677
89.407317	2609.291008	22.430695
89.450461	2619.109843	22.435712
89.809056	2595.548152	22.440730
89.171147	2620.136380	22.445747
89.580617	2630.874151	22.450765
89.810219	2641.108223	22.455783
89.707229	2639.043362	22.460800
90.082340	2640.086292	22.465818
89.941629	2656.078820	22.470835
90.762759	2667.511929	22.475853
90.676725	2657.947709	22.480871
90.792705	2668.155104	22.485888
91.257410	2661.912646	22.490906
90.819221	2664.261742	22.495923
90.820321	2659.751098	22.500941
91.016744	2665.204764	22.505959
90.792731	2673.368089	22.510976
90.778990	2669.003192	22.515994
90.712341	2688.313219	22.521011
91.372365	2691.242020	22.526029
91.547644	2690.913340	22.531047
91.485884	2694.516494	22.536064
91.534283	2690.949539	22.541082
91.483314	2703.734185	22.546099
91.852449	2711.285966	22.551117
92.365804	2714.315381	22.556135
92.018037	2723.435540	22.561152
92.409114	2726.625705	22.566170
91.982137	2719.482009	22.571187
91.712262	2731.704857	22.576205
92.517060	2717.469463	22.581223
92.580320	2720.109503	22.586240
92.807276	2705.315707	22.591258
92.914270	2711.427434	22.596275
92.664236	2714.808175	22.601293
93.136728	2715.286235	22.606311
93.081147	2724.527394	22.611328
93.384825	2723.385419	22.616346
93.271877	2733.532070	22.621363
93.522046	2733.037481	22.626381
93.627538	2732.968742	22.631399
93.447310	2737.498906	22.636416
93.445124	2726.318327	22.641434
93.372361	2733.986050	22.646451
93.458286	2736.755017	22.651469
93.759304	2731.025966	22.656487
93.383816	2719.429154	22.661504
93.811841	2729.198240	22.666522
93.814229	2751.140870	22.671539
93.767031	2756.935595	22.676557
94.127541	2762.402337	22.681575
94.438961	2759.106453	22.686592
94.425680	2749.097700	22.691610
94.428150	2760.385463	22.696627
94.391575	2759.179639	22.701645
94.562358	2761.199198	22.706663
94.585428	2783.404189	22.711680
94.858867	2782.602227	22.716698
94.776695	2790.481757	22.721715
94.705095	2790.001361	22.726733
95.182220	2792.245092	22.731751
94.869587	2795.518091	22.736768
95.219905	2808.771130	22.741786
95.408411	2809.472094	22.746803
95.647855	2815.816292	22.751821
95.481323	2814.752009	22.756839
95.081419	2819.079927	22.761856
95.558101	2812.421083	22.766874
95.566793	2831.834975	22.771891
95.556235	2851.211917	22.776909
96.030258	2839.487238	22.781927
95.490393	2841.876979	22.786944
95.979494	2857.415663	22.791962
96.005981	2862.953383	22.796979
96.392251	2862.429214	22.801997
96.716554	2863.557717	22.807015
96.605556	2862.289382	22.812032
96.936159	2870.151530	22.817050
97.033468	2890.462616	22.822067
96.955122	2887.437005	22.827085
97.373432	2884.650177	22.832103
97.852486	2881.269089	22.837120
97.902519	2882.089784	22.842138
98.052210	2872.666194	22.847155
97.766503	2853.646566	22.852173
97.725164	2853.115895	22.857191
97.715644	2854.163345	22.862208
97.547794	2858.126569	22.867226
97.781782	2866.677478	22.872243
97.753886	2884.238525	22.877261
98.340547	2875.326557	22.882279
98.229813	2885.305627	22.887296
98.128225	2883.663315	22.892314
98.306351	2873.285469	22.897331
98.444462	2877.897316	22.902349
98.706174	2887.531395	22.907367
98.499235	2893.907262	22.912384
98.664581	2902.893922	22.917402
98.808462	2901.635828	22.922419
98.645137	2902.250452	22.927437
98.914735	2897.863080	22.932455
98.586715	2908.003653	22.937472
98.941780	2919.660414	22.942490
98.870500	2924.438758	22.947507
98.942357	2925.866055	22.952525
99.327142	2938.772188	22.957543
99.373825	2954.564382	22.962560
99.550991	2954.101927	22.967578
99.864000	2946.658299	22.972595
99.918189	2953.950051	22.977613
99.956184	2964.074273	22.982631
100.140024	2971.215483	22.987648
100.532928	2982.517235	22.992666
100.499989	2972.768661	22.997683
100.470987	2979.078549	23.002701
100.835660	2978.257565	23.007719
100.737554	2972.931764	23.012736
100.835689	2976.675877	23.017754
101.001326	2969.267613	23.022771
100.789894	2973.988033	23.027789
101.004399	2956.689083	23.032807
100.842199	2978.896230	23.037824
101.056454	2998.043696	23.042842
101.526849	2997.584359	23.047859
101.406061	3000.453276	23.052877
101.668041	2991.815749	23.057895
101.673650	3004.730265	23.062912
101.487327	3000.291041	23.067930
101.438549	3001.774103	23.072947
101.564190	3017.143490	23.077965
101.893029	3021.627411	23.082983
102.072627	3031.688123	23.088000
101.742221	3032.666961	23.093018
102.329287	3033.854023	23.098035
102.276296	3033.102445	23.103053
102.698820	3054.112338	23.108071
102.756881	3054.739597	23.113088
102.557637	3060.939465	23.118106
103.147651	3050.802089	23.123123
103.084569	3056.561363	23.128141
103.211572	3048.645293	23.133159
103.326086	3060.449384	23.138176
103.303053	3049.733415	23.143194
103.152534	3048.813314	23.148211
103.303437	3053.678602	23.153229
103.666965	3070.561033	23.158247
104.022609	3070.345843	23.163264
103.953494	3077.745427	23.168282
104.356006	3072.906926	23.173299
103.944177	3067.184131	23.178317
104.663585	3064.796319	23.183335
104.912162	3066.898731	23.188352
104.817852	3056.935056	23.193370
104.991692	3061.519796	23.198387
105.059193	3065.561107	23.203405
104.650136	3043.985351	23.208423
104.657253	3051.422717	23.213440
104.444842	3055.545710	23.218458
105.003870	3059.330610	23.223475
104.866580	3055.440331	23.228493
105.099832	3051.877786	23.233511
105.210278	3057.398159	23.238528
105.257048	3081.040942	23.243546
105.487802	3081.741236	23.248563
105.253925	3091.097505	23.253581
105.319086	3094.693164	23.258599
105.487619	3099.979159	23.263616
105.840906	3119.619532	23.268634
105.475134	3110.175860	23.273651
105.754930	3121.792457	23.278669
105.880827	3123.374616	23.283687
105.865418	3135.578566	23.288704
106.327702	3140.088108	23.293722
106.633500	3145.663631	23.298739
106.262807	3149.260460	23.303757
106.778616	3162.362052	23.308775
106.935598	3174.778484	23.313792
106.973187	3182.169541	23.318810
107.204766	3173.165689	23.323827
107.247546	3181.947575	23.328845
107.773193	3179.669320	23.333863
107.542308	3181.614367	23.338880
107.484351	3176.733815	23.343898
107.772294	3179.522235	23.348915
107.512978	3173.313977	23.353933
108.008940	3173.882267	23.358951
107.862444	3189.683001	23.363968
107.886385	3196.048400	23.368986
108.448115	3189.532819	23.374003
108.255903	3197.196099	23.379021
108.395907	3190.972243	23.384039
108.322167	3191.012644	23.389056
108.222125	3194.998606	23.394074
108.429995	3197.820731	23.399091
108.588625	3201.996228	23.404109
108.765291	3215.391693	23.409127
108.988878	3216.266795	23.414144
108.825281	3231.801902	23.419162
109.143361	3220.690877	23.424179
109.027738	3224.184159	23.429197
109.429230	3241.497499	23.434215
109.603077	3240.013960	23.439232
109.611433	3250.044451	23.444250
109.596586	3250.066853	23.449267
109.918640	3253.204757	23.454285
109.705687	3241.381093	23.459303
109.928588	3251.595812	23.464320
109.820524	3270.286654	23.469338
110.503803	3274.958927	23.474355
110.030190	3281.750268	23.479373
110.321849	3270.616015	23.484391
110.607423	3278.757065	23.489408
110.533189	3282.258088	23.494426
111.134095	3290.611205	23.499443
110.925468	3296.807600	23.504461
111.122786	3300.302337	23.509479
111.235339	3288.273674	23.514496
111.203481	3296.194357	23.519514
111.460360	3290.360588	23.524531
111.523730	3310.239655	23.529549
111.321265	3320.027474	23.534567
111.477626	3316.793316	23.539584
111.726150	3328.885304	23.544602
112.037906	3318.905937	23.549619
112.299321	3328.543884	23.554637
112.553311	3338.101569	23.559655
112.628355	3344.603070	23.564672
112.340093	3350.322891	23.569690
112.501294	3337.043658	23.574707
112.515423	3347.743322	23.579725
112.690686	3356.887659	23.584743
112.981471	3339.583946	23.589760
113.018615	3352.917548	23.594778
113.146230	3353.180971	23.599795
113.562622	3366.605852	23.604813
113.765482	3363.464391	23.609831
113.607851	3367.719750	23.614848
113.602512	3370.730284	23.619866
113.483510	3366.889267	23.624883
113.663139	3365.430745	23.629901
113.484115	3359.167413	23.634919
113.780082	3370.402006	23.639936
113.455398	3389.170910	23.644954
113.742729	3398.965245	23.649971
114.029589	3401.815301	23.654989
114.318564	3418.537993	23.660007
114.649297	3427.053149	23.665024
114.541098	3423.440644	23.670042
114.715267	3418.606304	23.675059
114.950584	3431.404873	23.680077
115.182735	3445.010657	23.685095
115.508838	3438.838234	23.690112
115.435954	3441.727268	23.695130
115.961567	3436.026989	23.700147
115.721315	3437.783854	23.705165
115.737082	3431.319412	23.710183
116.050235	3433.278529	23.715200
115.907051	3450.273449	23.720218
115.943132	3436.332139	23.725235
115.939039	3440.488133	23.730253
116.214159	3437.829198	23.735271
116.463736	3428.705297	23.740288
116.149852	3438.763566	23.745306
116.335287	3454.046736	23.750323
116.170854	3469.402693	23.755341
116.288514	3463.367851	23.760359
116.919511	3470.686582	23.765376
116.664900	3481.429170	23.770394
116.912055	3501.193469	23.775411
117.368442	3497.764423	23.780429
117.306098	3502.718238	23.785447
117.428534	3496.788892	23.790464
117.439965	3505.991490	23.795482
117.797421	3519.512068	23.800499
118.081402	3513.168625	23.805517
117.639575	3527.628360	23.810535
118.222727	3509.930876	23.815552
117.997095	3523.365918	23.820570
118.130009	3517.361605	23.825587
118.494793	3518.187017	23.830605
118.527235	3542.797034	23.835623
118.624324	3544.150141	23.840640
118.629315	3538.692543	23.845658
118.561041	3542.254450	23.850675
118.817607	3552.073651	23.855693
118.983794	3564.127067	23.860711
118.964795	3572.033168	23.865728
119.003365	3579.699054	23.870746
118.986078	3585.810009	23.875763
119.461548	3590.662780	23.880781
119.288057	3609.523895	23.885799
120.085325	3609.926670	23.890816
120.043345	3603.176030	23.895834
120.439214	3598.085318	23.900851
120.484632	3621.869698	23.905869
120.643975	3636.314056	23.910887
120.766751	3625.404699	23.915904
120.462731	3623.377254	23.920922
120.713270	3628.127834	23.925939
121.156120	3623.678955	23.930957
120.984934	3627.553160	23.935975
121.188521	3618.695409	23.940992
120.857250	3620.928355	23.946010
120.974071	3627.339607	23.951027
121.395105	3644.295840	23.956045
121.441654	3648.171474	23.961063
121.348728	3658.120933	23.966080
121.480605	3667.897032	23.971098
121.928260	3674.844975	23.976115
122.236677	3673.623018	23.981133
122.260855	3681.707867	23.986151
122.404927	3674.442989	23.991168
122.641628	3673.510835	23.996186
122.502065	3677.031796	24.001203
122.931819	3676.152782	24.006221
122.777075	3690.545545	24.011239
123.037209	3689.540227	24.016256
123.077448	3695.156680	24.021274
123.070891	3688.042276	24.026291
122.920397	3692.802842	24.031309
123.021458	3701.549802	24.036327
123.386985	3708.447158	24.041344
123.482860	3711.963082	24.046362
123.835420	3712.014933	24.051379
123.749232	3723.882615	24.056397
123.772146	3721.753104	24.061415
124.018641	3719.550034	24.066432
124.135034	3736.190957	24.071450
124.063771	3738.215602	24.076467
124.825197	3743.797159	24.081485
124.220892	3752.548888	24.086503
124.443022	3742.095475	24.091520
124.776507	3765.623815	24.096538
124.723521	3772.834055	24.101555
124.856459	3778.293095	24.106573
124.793472	3781.502212	24.111591
125.246176	3780.334359	24.116608
125.617406	3804.295893	24.121626
125.387655	3798.899039	24.126643
125.671984	3802.420066	24.131661
125.483092	3809.972074	24.136679
125.919775	3802.276499	24.141696
125.814434	3830.714887	24.146714
125.929864	3836.046917	24.151731
126.184770	3830.682569	24.156749
126.261874	3833.593743	24.161767
126.445645	3836.572726	24.166784
126.827124	3852.510123	24.171802
126.707951	3850.030445	24.176819
127.495597	3842.399302	24.181837
127.323431	3843.758736	24.186855
127.631056	3841.357358	24.191872
127.978596	3849.027836	24.196890
127.674256	3839.964120	24.201907
127.618142	3845.686707	24.206925
127.494465	3858.172504	24.211943
127.507764	3859.437908	24.216960
127.778040	3865.742799	24.221978
127.537190	3882.903938	24.226995
128.162599	3903.701539	24.232013
128.221491	3906.915740	24.237031
128.414532	3907.982548	24.242048
128.508393	3916.470578	24.247066
128.801737	3935.869920	24.252083
128.887082	3930.126069	24.257101
129.155495	3947.079505	24.262119
129.269362	3926.691724	24.267136
129.289238	3931.719492	24.272154
129.188001	3946.275307	24.277171
129.785469	3954.670695	24.282189
129.825394	3959.327436	24.287207
129.775442	3964.173837	24.292224
129.570238	3966.904907	24.297242
129.895616	3970.332574	24.302259
130.378409	3978.980786	24.307277
130.316859	3993.577332	24.312295
130.471558	3988.738160	24.317312
130.799422	3988.080694	24.322330
130.404537	3993.295915	24.327347
131.155777	3987.859344	24.332365
130.764968	4010.361255	24.337383
131.192357	4015.012259	24.342400
131.546277	4014.783567	24.347418
131.407563	4017.645002	24.352435
131.342894	4014.302336	24.357453
131.389908	4013.647181	24.362471
131.399136	4033.052644	24.367488
132.179678	4031.109721	24.372506
131.978188	4042.097072	24.377523
132.249331	4024.593872	24.382541
132.166004	4046.487141	24.387559
132.296225	4060.700480	24.392576
132.923496	4065.136971	24.397594
132.729090	4054.854147	24.402611
133.082816	4057.955094	24.407629
132.839784	4065.323648	24.412647
133.333538	4063.763156	24.417664
133.199551	4064.249350	24.422682
133.193627	4061.601316	24.427699
133.550349	4080.595869	24.432717
133.505730	4087.415887	24.437735
133.301999	4101.156476	24.442752
134.203367	4086.468442	24.447770
133.825383	4100.861856	24.452787
134.087135	4096.793171	24.457805
134.112623	4102.895687	24.462823
134.153162	4102.475462	24.467840
134.260313	4106.154184	24.472858
134.269216	4133.556110	24.477875
134.523382	4136.193195	24.482893
134.711501	4140.100680	24.487911
134.661082	4137.670621	24.492928
135.006787	4153.410296	24.497946
134.836606	4163.083463	24.502963
135.191337	4167.062640	24.507981
135.569842	4186.100574	24.512999
135.902601	4199.749454	24.518016
136.136378	4188.111496	24.523034
136.002075	4202.961213	24.528051
136.262855	4187.122197	24.533069
136.231194	4198.568226	24.538087
136.627660	4206.357573	24.543104
136.910898	4215.871204	24.548122
136.867734	4217.611730	24.553139
136.855627	4205.017504	24.558157
137.036582	4213.558631	24.563175
137.243161	4217.911132	24.568192
137.449611	4230.441106	24.573210
137.312402	4249.851351	24.578227
137.814243	4244.836231	24.583245
137.690811	4249.915736	24.588263
137.793880	4245.896462	24.593280
137.980685	4245.734752	24.598298
137.695088	4271.932782	24.603315
138.168005	4272.754938	24.608333
137.921018	4278.122594	24.613351
138.419790	4288.134928	24.618368
138.709358	4292.850523	24.623386
138.551366	4308.312939	24.628403
138.895315	4310.764346	24.633421
138.960058	4305.915135	24.638439
139.121559	4323.662665	24.643456
139.401326	4327.747581	24.648474
139.612435	4326.038878	24.653491
139.728791	4334.294276	24.658509
139.965934	4326.182579	24.663527
140.162854	4343.900656	24.668544
140.416857	4351.427777	24.673562
140.244965	4360.492268	24.678579
140.928135	4354.343954	24.683597
140.947134	4354.796611	24.688615
141.087223	4356.145047	24.693632
140.646070	4354.328752	24.698650
140.759007	4352.600046	24.703667
140.608138	4356.149800	24.708685
140.792759	4366.006210	24.713703
140.998410	4381.829104	24.718720
141.581326	4379.293177	24.723738
141.532327	4393.863614	24.728755
141.747939	4408.961234	24.733773
141.892476	4420.172002	24.738791
141.652862	4418.989360	24.743808
142.114595	4411.233441	24.748826
141.963951	4430.402812	24.753843
142.174952	4435.567675	24.758861
142.717776	4432.648188	24.763879
142.740586	4441.374240	24.768896
143.018269	4435.215726	24.773914
142.868273	4436.482567	24.778931
143.266548	4462.304912	24.783949
143.135271	4459.152300	24.788967
143.349136	4462.215413	24.793984
143.514507	4461.654467	24.799002
143.655169	4472.034376	24.804019
143.743856	4478.160062	24.809037
144.134716	4486.329631	24.814055
144.302542	4486.519498	24.819072
144.862265	4477.639424	24.824090
144.956058	4482.892965	24.829107
144.873508	4469.440041	24.834125
145.295533	4473.493222	24.839143
145.070949	4479.221830	24.844160
145.095165	4468.898671	24.849178
145.253126	4478.769007	24.854195
145.024087	4492.844455	24.859213
145.661493	4494.287904	24.864231
145.412354	4504.815318	24.869248
145.841626	4496.773367	24.874266
145.812456	4516.255072	24.879283
145.882027	4517.664390	24.884301
145.959197	4521.128074	24.889319
146.235355	4526.546389	24.894336
146.327428	4532.811702	24.899354
146.312178	4562.171236	24.904371
146.317040	4546.691483	24.909389
146.533881	4565.363660	24.914407
146.422540	4572.387839	24.919424
147.282139	4575.755718	24.924442
147.209911	4587.846567	24.929459
147.729187	4593.013305	24.934477
148.127208	4594.977055	24.939495
148.386864	4591.562565	24.944512
148.829808	4584.844765	24.949530
148.815759	4584.609148	24.954547
149.200849	4592.918711	24.959565
149.047119	4582.434317	24.964583
148.845639	4584.756587	24.969600
149.042869	4590.686420	24.974618
148.937006	4585.415680	24.979635
149.003753	4595.414948	24.984653
149.123505	4585.124747	24.989671
148.875677	4599.086853	24.994688
149.658775	4613.188096	24.999706
149.431643	4624.044650	25.004723
149.623130	4616.647870	25.009741
150.068674	4636.805664	25.014759
149.601707	4649.962240	25.019776
149.908476	4649.077119	25.024794
149.883826	4663.307936	25.029811
150.150980	4672.481964	25.034829
150.460497	4674.459167	25.039847
150.319136	4688.172644	25.044864
150.901519	4715.865900	25.049882
150.657472	4715.953342	25.054899
150.896173	4735.515478	25.059917
151.342108	4743.272906	25.064935
151.223356	4746.833978	25.069952
151.427925	4759.207986	25.074970
151.728631	4769.270684	25.079987
151.538507	4780.401566	25.085005
152.236558	4773.164335	25.090023
152.454555	4761.204127	25.095040
152.767778	4772.898730	25.100058
152.631995	4786.778312	25.105075
152.711770	4789.810493	25.110093
152.759297	4785.513623	25.115111
153.099578	4797.555374	25.120128
153.049339	4794.364891	25.125146
153.252139	4815.169762	25.130163
153.403464	4813.237797	25.135181
153.390198	4811.975201	25.140199
153.511988	4824.781474	25.145216
153.738947	4833.725607	25.150234
153.769867	4850.759038	25.155251
153.886617	4845.501824	25.160269
154.076544	4865.379292	25.165287
154.647823	4881.980927	25.170304
155.022200	4884.991616	25.175322
154.864942	4883.037003	25.180339
155.334512	4906.401267	25.185357
155.529413	4907.250892	25.190375
155.536202	4913.595810	25.195392
155.709582	4902.833511	25.200410
155.646668	4907.672503	25.205427
155.613735	4924.074782	25.210445
156.106307	4934.142895	25.215463
155.960488	4938.959371	25.220480
156.103678	4942.014177	25.225498
156.185408	4943.683356	25.230515
156.524709	4962.490118	25.235533
156.768354	4958.610833	25.240551
156.794771	4967.143261	25.245568
156.835400	4979.363809	25.250586
156.874263	4987.717404	25.255603
156.954547	4997.485147	25.260621
157.809242	5009.321975	25.265639
157.757471	5022.020461	25.270656
158.001941	5011.147121	25.275674
158.057047	5005.585051	25.280691
158.462503	5030.801590	25.285709
158.705241	5048.733784	25.290727
158.678961	5045.477081	25.295744
158.940028	5052.721068	25.300762
159.249051	5042.381576	25.305779
158.984363	5046.745244	25.310797
159.133581	5048.810799	25.315815
159.256066	5073.342997	25.320832
159.436471	5073.813103	25.325850
159.537712	5068.752883	25.330867
159.374284	5086.356526	25.335885
160.259817	5088.524855	25.340903
160.144116	5090.647576	25.345920
160.290699	5100.219765	25.350938
160.496411	5109.441215	25.355955
160.587522	5121.006622	25.360973
160.662584	5127.195845	25.365991
160.786122	5133.052227	25.371008
160.840586	5134.530638	25.376026
161.138652	5153.727945	25.381043
161.033367	5156.988432	25.386061
161.526144	5154.636980	25.391079
161.406041	5183.862237	25.396096
161.627422	5188.183822	25.401114
161.853757	5193.140873	25.406131
162.016367	5213.873380	25.411149
163.195793	5205.321255	25.416167
163.268515	5209.789076	25.421184
163.264469	5208.285137	25.426202
163.415346	5208.960934	25.431219
163.283565	5203.993508	25.436237
163.839196	5197.256436	25.441255
163.412352	5196.499195	25.446272
163.741730	5195.400052	25.451290
163.746255	5191.925216	25.456307
163.641642	5210.130758	25.461325
163.658301	5198.646833	25.466343
163.773214	5224.120374	25.471360
163.709613	5219.936245	25.476378
164.295301	5234.073035	25.481395
164.062676	5258.493709	25.486413
164.411994	5255.122534	25.491431
164.415276	5282.425821	25.496448
164.542997	5292.006364	25.501466
164.976483	5305.270243	25.506483
165.209373	5321.056909	25.511501
165.287824	5324.508749	25.516519
165.569378	5337.925332	25.521536
165.342129	5361.221142	25.526554
165.904635	5361.957686	25.531571
165.964493	5389.749503	25.536589
166.320636	5383.228011	25.541607
166.594923	5385.626922	25.546624
167.132404	5399.541488	25.551642
167.290002	5398.180920	25.556659
167.467658	5406.500782	25.561677
167.702243	5410.625344	25.566695
167.900849	5403.967651	25.571712
167.817463	5399.267000	25.576730
168.064430	5410.173730	25.581747
168.031691	5430.111939	25.586765
168.581377	5429.531953	25.591783
168.173052	5423.847861	25.596800
168.324533	5430.000164	25.601818
168.673395	5440.904648	25.606835
168.333040	5467.935079	25.611853
168.696856	5464.962692	25.616871
168.919598	5481.765093	25.621888
168.908559	5491.333642	25.626906
169.791656	5496.950866	25.631923
169.537440	5515.118087	25.636941
169.681665	5518.377190	25.641959
169.883912	5531.910600	25.646976
169.997367	5538.206253	25.651994
170.316573	5540.565085	25.657011
170.129172	5560.792039	25.662029
170.803506	5571.723554	25.667047
171.095931	5577.464786	25.672064
171.046288	5576.873573	25.677082
171.420310	5568.824063	25.682100
171.569730	5590.078209	25.687117
172.096045	5600.020298	25.692135
172.023300	5602.502571	25.697152
172.070313	5612.083258	25.702170
172.667618	5605.789183	25.707188
172.441525	5611.833451	25.712205
172.404984	5601.610145	25.717223
172.710958	5601.353529	25.722240
172.859328	5620.687970	25.727258
173.092373	5626.517781	25.732276
173.194803	5634.994700	25.737293
173.790579	5629.266294	25.742311
173.710244	5632.710181	25.747328
173.342328	5652.792255	25.752346
173.681051	5660.552895	25.757364
173.794058	5661.305451	25.762381
173.858313	5656.736647	25.767399
174.099752	5679.067974	25.772416
174.274474	5677.316708	25.777434
174.755340	5681.097068	25.782452
174.793805	5695.167195	25.787469
175.204804	5705.024849	25.792487
175.166726	5718.042545	25.797504
175.173073	5717.713765	25.802522
175.187242	5720.541191	25.807540
175.353787	5729.744279	25.812557
175.285337	5737.530102	25.817575
175.813551	5751.798530	25.822592
175.994099	5770.439559	25.827610
176.247135	5772.489239	25.832628
176.219877	5781.886999	25.837645
176.626199	5802.986373	25.842663
176.541503	5798.346457	25.847680
176.970653	5825.890997	25.852698
177.427065	5828.416206	25.857716
177.541367	5828.807483	25.862733
178.041173	5813.324631	25.867751
178.511120	5804.447229	25.872768
178.641952	5807.893671	25.877786
179.009676	5801.426794	25.882804
178.718699	5810.451159	25.887821
178.771618	5819.868377	25.892839
179.150003	5822.953403	25.897856
179.132677	5826.562143	25.902874
179.233465	5821.884878	25.907892
179.231544	5821.470049	25.912909
179.667450	5839.107812	25.917927
179.867104	5859.621246	25.922944
179.672360	5865.412365	25.927962
179.910894	5862.460999	25.932980
179.829976	5868.060847	25.937997
180.083047	5880.604528	25.943015
180.124605	5892.227914	25.948032
180.206814	5916.339681	25.953050
180.694579	5921.826291	25.958068
180.847810	5938.756828	25.963085
180.961822	5952.203197	25.968103
180.918569	5954.221924	25.973120
181.016054	5983.448550	25.978138
181.373947	5981.827246	25.983156
181.633991	6006.321245	25.988173
181.698369	6015.620922	25.993191
182.335181	6027.593366	25.998208
182.716032	6055.695586	26.003226
183.008154	6040.690988	26.008244
183.055271	6054.429643	26.013261
183.459045	6059.456880	26.018279
183.420682	6073.863318	26.023296
183.697319	6084.239158	26.028314
183.772895	6073.219735	26.033332
183.633549	6075.217341	26.038349
183.629384	6087.623348	26.043367
184.437474	6095.399187	26.048384
184.176064	6108.787229	26.053402
184.346567	6119.351521	26.058420
185.034583	6128.640363	26.063437
184.740788	6151.499845	26.068455
185.055631	6150.133707	26.073472
185.148827	6166.863746	26.078490
185.216095	6178.970575	26.083508
185.424651	6183.771799	26.088525
185.543916	6197.407304	26.093543
186.026980	6196.948165	26.098560
185.799770	6210.565326	26.103578
186.321514	6220.955886	26.108596
186.353160	6225.405976	26.113613
186.295754	6237.848462	26.118631
186.991009	6251.829075	26.123648
186.874344	6256.500562	26.128666
187.351661	6256.611756	26.133684
187.747048	6278.035284	26.138701
187.499192	6279.342065	26.143719
188.091250	6286.669363	26.148736
187.918408	6290.875260	26.153754
188.184466	6279.130403	26.158772
188.700488	6306.183797	26.163789
188.698582	6311.495505	26.168807
188.829835	6302.819873	26.173824
188.625261	6321.093227	26.178842
189.188531	6336.757422	26.183860
189.369218	6338.126495	26.188877
189.744482	6351.726138	26.193895
189.660561	6367.936742	26.198912
189.509636	6367.194095	26.203930
189.695662	6384.424864	26.208948
190.503870	6389.829557	26.213965
190.797965	6393.729944	26.218983
191.182833	6389.749404	26.224000
191.197050	6407.993797	26.229018
191.232655	6410.279129	26.234036
191.540556	6418.970992	26.239053
191.644241	6423.487202	26.244071
191.767821	6425.960398	26.249088
191.647980	6453.801905	26.254106
191.905269	6447.688505	26.259124
192.299945	6464.457253	26.264141
191.879285	6479.768323	26.269159
192.584988	6485.938152	26.274176
192.417382	6502.482464	26.279194
192.840579	6510.369360	26.284212
193.213417	6522.066845	26.289229
193.285933	6539.960752	26.294247
193.598495	6543.192650	26.299264
193.385473	6557.333059	26.304282
193.866164	6572.158222	26.309300
193.815791	6574.900386	26.314317
194.054544	6605.817350	26.319335
194.899378	6597.276458	26.324352
195.137138	6593.135099	26.329370
195.470514	6603.316835	26.334388
195.544991	6634.687063	26.339405
195.536816	6635.284854	26.344423
195.853088	6632.103137	26.349440
195.965480	6640.038302	26.354458
196.203598	6644.297674	26.359476
196.253341	6651.191027	26.364493
196.263214	6668.672515	26.369511
196.453398	6665.723477	26.374528
196.480837	6681.500965	26.379546
196.759923	6690.114260	26.384564
197.267369	6694.437040	26.389581
196.920138	6725.734579	26.394599
197.348864	6732.448005	26.399616
197.441153	6747.849419	26.404634
197.720833	6746.943462	26.409652
197.858635	6761.248180	26.414669
198.158090	6768.543721	26.419687
198.561094	6759.304726	26.424704
198.948986	6775.997748	26.429722
199.278369	6788.569713	26.434740
199.934772	6792.039399	26.439757
199.286956	6795.413490	26.444775
199.884101	6794.936275	26.449792
199.807382	6800.707842	26.454810
199.779322	6802.850964	26.459828
199.917921	6813.077619	26.464845
200.378976	6824.948982	26.469863
200.343489	6821.259880	26.474880
199.943887	6843.436918	26.479898
200.417925	6846.337414	26.484916
200.920356	6872.965598	26.489933
200.967213	6888.703070	26.494951
201.423212	6882.532257	26.499968
201.493104	6906.481795	26.504986
201.376634	6920.104899	26.510004
201.926619	6928.020674	26.515021
201.988882	6949.158357	26.520039
202.090618	6952.326729	26.525056
202.579109	6974.854958	26.530074
202.919233	6984.415224	26.535092
203.237282	6980.798408	26.540109
203.667268	7002.552713	26.545127
203.618691	7007.039119	26.550144
204.179952	7006.342584	26.555162
203.952891	7002.293671	26.560180
204.271172	7017.489470	26.565197
204.649252	7023.519904	26.570215
204.751605	7014.098890	26.575232
205.129225	7026.417355	26.580250
204.941758	7035.031531	26.585268
205.404530	7044.642451	26.590285
205.243710	7060.307298	26.595303
205.245477	7064.523928	26.600320
205.696789	7082.556696	26.605338
205.870555	7092.364247	26.610356
206.168059	7098.645870	26.615373
206.141988	7105.918171	26.620391
206.642780	7129.945706	26.625408
206.734493	7148.144286	26.630426
206.815976	7155.335833	26.635444
207.248703	7154.268317	26.640461
207.183212	7185.657255	26.645479
207.680016	7171.978699	26.650496
207.869563	7202.270179	26.655514
208.051769	7214.302896	26.660532
208.441058	7210.868790	26.665549
208.508325	7226.826112	26.670567
208.802500	7234.964666	26.675584
209.501269	7239.771066	26.680602
209.118811	7241.051333	26.685620
209.488227	7250.005998	26.690637
209.396803	7275.335027	26.695655
209.621452	7280.869531	26.700672
209.740584	7292.978100	26.705690
209.745787	7305.402420	26.710708
210.626786	7316.758999	26.715725
210.591097	7326.148442	26.720743
210.427036	7340.329504	26.725760
210.560218	7355.263231	26.730778
210.882902	7361.252543	26.735796
211.438074	7375.408526	26.740813
211.789517	7397.550459	26.745831
212.078038	7394.781936	26.750848
211.985766	7403.828722	26.755866
212.195916	7426.227167	26.760884
212.314927	7427.343472	26.765901
212.553444	7452.752949	26.770919
212.785404	7453.922265	26.775936
213.013970	7469.179005	26.780954
213.247418	7486.460640	26.785972
213.270202	7485.182815	26.790989
213.340229	7504.147778	26.796007
213.467956	7512.659731	26.801024
214.122624	7519.161319	26.806042
214.624734	7539.631699	26.811060
214.638475	7547.585196	26.816077
214.897771	7548.064007	26.821095
214.857196	7564.055240	26.826112
214.899109	7576.592636	26.831130
215.329683	7590.155861	26.836148
215.676452	7588.411796	26.841165
215.512157	7609.168006	26.846183
215.983345	7614.536666	26.851200
216.511517	7619.961284	26.856218
216.608792	7637.727905	26.861236
216.727102	7634.640132	26.866253
216.879958	7666.404289	26.871271
216.571621	7669.216041	26.876288
217.055338	7681.476535	26.881306
217.349077	7697.964777	26.886324
217.913401	7709.625210	26.891341
218.256988	7722.131780	26.896359
218.378222	7728.828706	26.901376
218.706057	7725.599970	26.906394
218.517959	7753.512541	26.911412
218.724533	7756.588144	26.916429
218.881614	7768.699471	26.921447
219.187319	7789.420006	26.926464
219.692267	7788.526393	26.931482
219.565968	7811.754405	26.936500
219.674948	7810.350471	26.941517
220.143545	7836.431400	26.946535
220.294033	7844.639692	26.951552
220.724796	7857.140629	26.956570
220.794446	7874.285142	26.961588
221.060788	7873.045806	26.966605
221.451283	7896.735947	26.971623
221.592225	7899.927174	26.976640
222.428766	7910.386565	26.981658
221.966971	7942.875833	26.986676
222.215428	7938.874129	26.991693
222.634709	7949.135484	26.996711
222.818169	7965.202736	27.001728
222.975741	7962.841683	27.006746
223.206252	7977.248755	27.011764
223.917055	7991.701716	27.016781
223.531854	7996.607899	27.021799
223.602817	8006.655900	27.026816
224.138963	8021.596140	27.031834
223.928597	8031.177111	27.036852
224.375418	8053.856329	27.041869
224.672691	8054.789641	27.046887
225.055952	8081.786901	27.051904
225.223883	8075.551381	27.056922
225.424568	8099.061317	27.061940
225.870823	8109.190725	27.066957
225.959127	8121.712224	27.071975
225.789012	8126.359224	27.076992
226.371314	8144.840204	27.082010
226.426191	8155.627388	27.087028
226.744256	8177.445128	27.092045
226.981383	8191.897772	27.097063
226.966820	8188.437243	27.102080
227.334233	8197.133650	27.107098
227.123210	8212.495242	27.112116
227.639943	8232.111104	27.117133
227.714866	8241.752184	27.122151
227.893136	8256.427271	27.127168
228.316985	8272.726064	27.132186
228.411952	8291.445260	27.137204
228.787781	8309.434408	27.142221
229.106548	8304.004043	27.147239
229.066383	8331.029155	27.152256
229.309727	8331.915472	27.157274
229.565822	8370.975602	27.162292
230.002913	8371.849601	27.167309
230.246392	8388.822601	27.172327
230.420236	8401.744486	27.177344
230.917577	8401.089966	27.182362
231.183142	8440.180995	27.187380
231.216198	8431.647232	27.192397
231.386608	8444.822552	27.197415
231.782543	8460.307004	27.202432
232.388447	8462.065994	27.207450
232.256947	8474.634327	27.212468
232.421456	8498.349318	27.217485
232.781427	8505.404101	27.222503
232.752453	8520.263327	27.227520
233.072218	8517.483935	27.232538
233.149748	8535.636834	27.237556
233.238033	8563.046756	27.242573
233.843806	8572.357735	27.247591
233.587922	8599.460690	27.252608
233.989370	8610.752516	27.257626
234.042369	8633.811118	27.262644
234.506697	8648.375507	27.267661
234.630057	8674.708621	27.272679
234.792338	8693.339192	27.277696
235.228886	8701.284062	27.282714
235.347728	8715.139206	27.287732
235.539335	8725.911277	27.292749
236.195565	8755.092860	27.297767
236.356512	8771.753816	27.302784
236.823192	8781.486455	27.307802
236.923061	8797.417920	27.312820
236.881799	8811.090083	27.317837
237.500665	8816.076374	27.322855
237.384743	8832.507458	27.327872
238.022445	8825.886843	27.332890
238.380061	8847.387847	27.337908
238.547053	8858.246778	27.342925
238.780327	8872.175310	27.347943
238.770657	8874.076224	27.352960
239.494068	8890.931086	27.357978
239.399595	8909.838267	27.362996
239.675720	8920.015210	27.368013
240.028490	8933.211217	27.373031
239.847459	8949.104964	27.378048
240.518360	8960.556527	27.383066
240.469450	8978.788322	27.388084
240.383551	8983.427959	27.393101
241.154996	8995.073243	27.398119
240.848191	9009.072222	27.403136
241.365291	9020.850917	27.408154
241.725023	9037.561228	27.413172
241.964923	9057.109640	27.418189
242.224904	9065.717941	27.423207
242.386387	9079.340297	27.428224
242.547497	9099.276710	27.433242
242.859016	9107.742614	27.438260
242.765405	9133.647610	27.443277
243.377413	9141.551898	27.448295
243.590122	9162.372301	27.453312
243.741081	9173.572798	27.458330
244.207892	9192.083538	27.463348
244.374850	9203.801279	27.468365
244.942875	9202.807380	27.473383
244.873614	9212.899005	27.478400
245.012831	9212.825069	27.483418
245.498215	9229.234409	27.488436
245.537839	9232.314254	27.493453
245.829786	9241.373435	27.498471
245.865505	9275.447591	27.503488
245.819011	9271.489561	27.508506
246.399542	9298.512228	27.513524
246.548730	9309.365745	27.518541
246.750653	9328.965664	27.523559
246.886464	9343.955970	27.528576
247.672177	9359.587217	27.533594
247.436619	9380.458336	27.538612
247.924989	9399.861357	27.543629
248.074591	9402.903372	27.548647
248.501489	9422.648193	27.553664
248.969643	9442.018372	27.558682
249.186766	9444.342682	27.563700
249.440339	9473.380226	27.568717
249.844244	9473.660343	27.573735
249.854260	9490.616380	27.578752
250.095880	9496.716787	27.583770
250.202625	9507.033943	27.588788
250.463322	9524.959999	27.593805
250.600181	9537.089409	27.598823
251.071700	9564.148656	27.603840
251.172160	9573.128599	27.608858
251.586367	9584.960949	27.613876
252.065065	9592.841803	27.618893
252.147727	9607.225946	27.623911
252.227632	9637.767054	27.628928
252.546112	9643.381411	27.633946
253.185698	9649.965940	27.638964
253.129905	9666.482473	27.643981
253.520328	9672.668640	27.648999
253.454679	9696.930726	27.654016
253.896560	9699.106086	27.659034
254.514232	9713.345219	27.664052
254.132285	9722.639683	27.669069
254.447289	9731.767017	27.674087
254.638092	9752.896654	27.679104
255.481340	9761.594079	27.684122
255.574396	9777.003827	27.689140
255.239548	9798.951363	27.694157
255.821985	9802.530842	27.699175
256.215725	9815.840547	27.704192
256.478073	9833.676091	27.709210
256.351021	9848.103765	27.714228
256.541903	9873.109869	27.719245
256.844808	9883.006519	27.724263
257.021023	9899.727577	27.729280
257.524816	9925.355560	27.734298
258.344425	9937.785237	27.739316
258.516798	9968.476333	27.744333
258.881633	9965.690824	27.749351
258.901024	9981.221644	27.754368
259.326339	9998.935135	27.759386
259.401928	10011.104176	27.764404
259.616764	10017.392746	27.769421
259.950872	10030.017715	27.774439
260.053822	10047.534025	27.779456
260.313619	10068.924446	27.784474
260.455318	10081.241737	27.789492
260.568505	10102.893530	27.794509
260.945123	10118.044073	27.799527
261.158602	10138.371723	27.804544
261.829705	10134.791974	27.809562
261.643603	10148.271803	27.814580
262.097555	10164.937800	27.819597
262.873118	10175.289832	27.824615
262.922749	10193.725723	27.829632
262.988111	10202.223429	27.834650
263.617330	10200.774299	27.839668
263.656915	10207.915074	27.844685
263.503119	10211.260232	27.849703
263.648308	10232.989625	27.854720
263.961033	10248.952757	27.859738
264.212354	10253.803301	27.864756
263.950210	10293.997516	27.869773
264.509480	10311.800294	27.874791
265.076156	10328.926781	27.879808
264.987898	10349.739381	27.884826
265.816144	10372.460517	27.889844
265.256700	10404.169800	27.894861
265.835010	10414.853919	27.899879
266.086665	10427.670067	27.904896
266.469231	10455.391471	27.909914
266.955823	10474.699206	27.914932
267.027263	10485.810570	27.919949
267.655793	10507.154837	27.924967
267.956175	10514.195944	27.929984
268.231523	10528.816917	27.935002
268.333704	10533.129737	27.940020
269.105074	10563.776581	27.945037
269.447944	10568.906713	27.950055
269.759437	10581.801326	27.955072
269.603053	10600.720738	27.960090
270.203423	10610.592329	27.965108
270.173502	10624.802992	27.970125
270.495681	10642.755596	27.975143
270.503014	10652.438450	27.980160
270.581641	10678.063050	27.985178
271.553223	10682.376433	27.990196
271.299460	10705.225603	27.995213
271.924264	10715.465829	28.000231
272.201111	10726.069197	28.005248
271.912506	10743.078263	28.010266
272.518729	10755.917235	28.015284
272.592555	10784.344842	28.020301
273.130364	10798.124702	28.025319
272.895250	10828.018238	28.030336
273.000335	10846.145583	28.035354
273.519902	10857.216255	28.040372
273.714266	10884.167557	28.045389
274.177658	10906.868596	28.050407
274.512152	10936.686346	28.055424
275.032021	10956.091576	28.060442
275.228219	10971.961245	28.065460
275.363291	10978.683252	28.070477
275.970038	10996.337155	28.075495
276.211347	11013.350339	28.080512
276.421045	11029.692859	28.085530
277.157821	11036.452553	28.090548
276.924901	11068.604707	28.095565
277.117501	11067.882277	28.100583
277.456184	11094.556428	28.105600
278.018034	11104.845119	28.110618
278.561639	11116.101853	28.115636
278.353735	11126.483069	28.120653
278.705485	11145.185251	28.125671
279.233234	11151.554131	28.130688
278.911826	11177.510313	28.135706
279.718125	11183.427481	28.140724
280.085071	11206.908235	28.145741
280.296725	11215.821890	28.150759
280.396958	11226.771456	28.155776
280.782784	11225.802032	28.160794
281.127640	11231.952223	28.165812
281.141958	11247.508744	28.170829
281.308450	11260.469614	28.175847
281.395514	11280.350873	28.180864
281.503761	11302.483288	28.185882
282.245354	11326.899653	28.190900
282.239278	11343.639734	28.195917
282.483235	11358.091763	28.200935
283.003239	11375.573712	28.205952
282.819768	11393.021435	28.210970
283.412962	11413.677927	28.215988
283.619970	11433.153544	28.221005
283.910925	11460.113491	28.226023
284.195448	11480.204226	28.231040
283.765829	11503.474328	28.236058
284.620057	11531.226024	28.241076
285.019292	11560.118824	28.246093
285.259516	11576.399349	28.251111
285.858916	11599.969898	28.256128
285.972776	11624.466004	28.261146
286.218485	11631.958593	28.266164
286.175536	11656.639790	28.271181
286.781038	11685.187557	28.276199
286.952457	11705.071161	28.281216
287.456293	11728.220457	28.286234
287.672399	11739.191407	28.291252
288.301274	11768.599681	28.296269
288.670885	11775.611789	28.301287
289.127762	11782.685900	28.306304
289.050263	11800.122859	28.311322
289.315724	11815.399732	28.316340
290.113624	11835.557356	28.321357
289.809120	11846.574999	28.326375
290.493454	11870.733012	28.331392
291.100641	11880.456159	28.336410
291.608628	11892.222736	28.341428
291.645894	11896.816081	28.346445
292.176334	11896.772040	28.351463
292.621902	11904.541347	28.356480
292.814009	11920.409481	28.361498
293.084327	11930.093775	28.366516
293.195439	11930.963546	28.371533
293.453504	11944.514880	28.376551
293.531001	11950.462934	28.381568
293.594389	11968.361304	28.386586
294.349716	11985.311082	28.391604
294.120794	11993.958410	28.396621
294.242048	12032.984388	28.401639
294.909012	12036.514967	28.406656
294.929897	12079.989903	28.411674
294.860058	12083.260126	28.416692
295.158692	12109.960703	28.421709
295.025610	12132.524101	28.426727
296.044727	12144.436465	28.431744
296.299755	12165.951800	28.436762
296.320698	12189.845677	28.441780
296.735955	12203.934555	28.446797
296.960444	12239.927396	28.451815
297.682812	12255.393124	28.456832
297.966855	12281.841140	28.461850
298.291936	12292.764528	28.466868
298.644409	12309.318749	28.471885
298.602476	12324.468841	28.476903
299.281813	12350.980869	28.481920
299.371368	12367.421807	28.486938
299.525776	12383.382499	28.491956
299.754071	12402.591850	28.496973
299.992904	12416.060885	28.501991
300.335857	12432.664076	28.507008
300.826434	12448.165134	28.512026
301.045297	12464.571416	28.517044
301.325236	12490.056138	28.522061
301.872125	12508.915177	28.527079
302.361435	12517.074628	28.532096
302.033335	12536.329577	28.537114
302.704167	12555.618053	28.542132
302.882667	12573.587891	28.547149
303.057476	12600.664268	28.552167
303.117144	12609.506902	28.557184
303.615322	12647.534561	28.562202
303.806152	12665.997233	28.567220
303.910445	12695.584473	28.572237
304.440214	12718.026575	28.577255
304.975698	12735.327821	28.582272
305.364180	12774.837731	28.587290
305.803044	12788.504084	28.592308
306.186996	12803.405423	28.597325
306.104502	12826.642139	28.602343
306.571748	12835.015755	28.607360
306.648034	12852.714436	28.612378
307.068420	12880.960860	28.617396
307.473739	12900.721422	28.622413
307.581326	12928.197081	28.627431
308.013697	12945.477770	28.632448
308.327006	12962.763967	28.637466
308.701394	12990.086928	28.642484
309.163479	13002.137657	28.647501
309.361750	13027.871505	28.652519
309.773148	13036.352148	28.657536
310.125632	13065.870700	28.662554
310.452241	13077.871384	28.667572
311.183949	13100.526472	28.672589
311.271112	13123.957766	28.677607
311.569358	13129.721666	28.682624
311.964116	13157.671843	28.687642
312.207991	13175.830095	28.692660
312.453386	13192.486429	28.697677
312.361848	13221.434141	28.702695
312.945859	13236.673130	28.707712
313.382449	13257.810899	28.712730
313.543030	13267.954552	28.717748
313.747691	13286.730800	28.722765
313.769594	13324.356557	28.727783
313.976646	13347.820368	28.732800
314.541658	13368.205911	28.737818
314.888301	13381.183637	28.742836
315.507823	13402.393798	28.747853
315.771165	13427.339102	28.752871
315.846643	13447.068158	28.757888
316.261267	13471.457502	28.762906
316.557715	13491.304533	28.767924
317.146048	13521.431021	28.772941
317.466490	13540.399591	28.777959
317.790705	13561.162376	28.782976
318.033552	13574.661656	28.787994
318.057741	13600.834878	28.793012
318.516770	13629.062045	28.798029
318.726920	13642.886669	28.803047
319.123738	13675.092036	28.808064
319.339987	13685.430032	28.813082
319.637845	13716.413255	28.818100
320.244800	13735.118835	28.823117
320.353381	13767.494917	28.828135
320.925152	13772.080858	28.833152
320.979272	13794.930806	28.838170
321.282411	13812.963374	28.843188
321.346429	13832.642791	28.848205
321.756391	13850.534839	28.853223
322.141688	13882.469907	28.858240
322.128678	13900.130906	28.863258
322.236802	13918.819832	28.868276
323.105155	13952.000497	28.873293
322.947860	13977.982118	28.878311
323.416350	14012.667693	28.883328
323.894634	14026.286037	28.888346
324.191597	14060.714827	28.893364
324.744034	14086.464335	28.898381
324.675930	14111.856256	28.903399
324.958028	14126.622788	28.908416
325.427743	14163.297191	28.913434
325.754934	14191.720461	28.918452
326.554433	14223.307271	28.923469
326.449402	14244.244276	28.928487
326.722390	14266.267652	28.933504
327.456274	14287.813074	28.938522
327.680674	14314.742298	28.943540
328.423233	14330.023891	28.948557
328.431473	14362.628900	28.953575
329.146865	14375.130478	28.958592
329.222074	14394.958435	28.963610
329.237687	14421.985363	28.968628
330.015132	14434.437339	28.973645
329.847121	14465.300396	28.978663
330.245317	14490.666301	28.983680
330.811283	14512.249218	28.988698
331.209306	14535.802965	28.993716
331.727693	14551.016218	28.998733
331.971882	14576.097251	29.003751
332.632490	14600.674585	29.008768
333.089902	14622.144783	29.013786
333.160190	14649.432534	29.018804
333.520019	14654.316916	29.023821
333.496619	14680.528105	29.028839
333.805963	14690.793055	29.033856
334.618579	14720.623124	29.038874
334.803740	14742.297624	29.043892
335.173009	14768.043805	29.048909
335.449529	14784.896774	29.053927
335.808945	14803.200080	29.058944
336.102586	14830.391350	29.063962
336.430179	14856.321057	29.068980
336.764697	14867.284815	29.073997
336.903988	14895.340077	29.079015
337.080979	14921.408234	29.084032
337.460077	14940.737516	29.089050
337.614759	14989.740650	29.094068
338.091270	14987.889281	29.099085
338.560894	15015.012389	29.104103
338.912375	15041.512081	29.109120
339.034901	15058.693352	29.114138
339.564752	15094.450611	29.119156
339.994048	15113.483410	29.124173
340.162109	15150.050704	29.129191
340.530376	15168.543648	29.134208
341.030402	15194.681799	29.139226
341.197714	15217.203007	29.144244
341.299500	15245.994730	29.149261
341.560109	15272.588608	29.154279
341.656603	15306.841976	29.159296
342.082999	15339.546909	29.164314
342.894016	15365.310887	29.169332
343.079543	15382.291399	29.174349
343.424461	15405.486405	29.179367
344.132617	15428.251084	29.184384
344.667503	15444.898154	29.189402
345.034665	15453.414169	29.194420
345.472527	15477.550535	29.199437
345.731919	15490.016415	29.204455
345.745236	15513.973967	29.209472
346.560906	15528.081548	29.214490
346.732587	15557.576189	29.219508
346.787758	15560.151940	29.224525
346.903844	15582.305457	29.229543
347.222379	15602.335809	29.234560
347.406230	15633.691387	29.239578
347.442404	15670.803285	29.244596
347.918305	15697.567167	29.249613
348.292325	15730.064050	29.254631
348.502650	15754.391286	29.259648
349.350469	15795.084003	29.264666
349.615392	15822.674096	29.269684
349.990341	15847.216978	29.274701
350.555867	15879.800722	29.279719
350.776639	15904.925492	29.284736
351.439447	15931.239662	29.289754
351.630930	15951.677554	29.294772
351.851359	15976.845044	29.299789
352.332008	16006.823723	29.304807
352.219717	16054.720508	29.309824
352.882125	16073.339248	29.314842
353.091703	16099.766388	29.319860
353.547949	16113.821958	29.324877
354.225619	16148.802190	29.329895
354.377325	16170.696878	29.334912
355.257487	16185.446856	29.339930
355.394838	16211.993279	29.344948
356.149444	16228.869628	29.349965
356.456843	16243.903405	29.354983
356.701259	16275.890080	29.360000
357.146352	16281.446451	29.365018
357.481820	16309.096632	29.370036
357.784444	16326.254211	29.375053
358.126887	16336.465875	29.380071
357.860574	16372.225072	29.385088
358.628406	16392.254667	29.390106
358.814707	16418.799643	29.395124
359.283573	16449.559654	29.400141
359.743293	16473.082369	29.405159
359.667475	16506.309173	29.410176
360.007700	16519.727040	29.415194
360.237567	16562.738132	29.420212
361.113503	16587.935390	29.425229
361.508507	16609.784167	29.430247
361.668558	16633.110748	29.435264
362.266287	16657.082176	29.440282
362.354315	16683.725772	29.445300
362.875978	16712.666634	29.450317
363.142423	16742.779766	29.455335
363.415769	16776.502642	29.460352
363.858845	16787.221227	29.465370
363.980914	16820.789510	29.470388
364.398547	16849.599646	29.475405
364.517163	16878.170804	29.480423
364.868502	16923.834270	29.485440
365.405257	16947.343363	29.490458
365.602223	16982.515116	29.495476
366.142633	17010.239799	29.500493
366.511373	17042.491132	29.505511
366.826546	17079.821762	29.510528
367.634945	17084.164669	29.515546
367.723143	17116.629561	29.520564
368.132245	17160.299799	29.525581
368.685990	17171.028724	29.530599
369.139635	17202.837637	29.535616
369.496065	17205.798894	29.540634
369.929356	17227.051118	29.545652
370.079257	17249.786048	29.550669
370.443675	17279.168411	29.555687
370.448606	17305.768424	29.560704
371.072875	17321.226839	29.565722
371.284289	17361.372909	29.570740
371.407472	17392.144509	29.575757
372.429168	17418.767452	29.580775
372.162622	17447.975370	29.585792
372.842390	17483.730424	29.590810
373.167834	17514.631184	29.595828
373.404103	17548.292417	29.600845
373.456805	17581.637286	29.605863
373.703042	17621.935854	29.610880
374.249037	17651.790109	29.615898
374.675633	17685.763788	29.620916
374.856103	17729.804304	29.625933
375.692526	17763.037409	29.630951
376.102039	17813.469582	29.635968
376.576133	17824.398085	29.640986
376.948601	17864.145214	29.646004
377.378505	17895.994066	29.651021
378.032124	17920.732022	29.656039
378.167604	17955.737899	29.661056
379.031593	17973.926724	29.666074
378.931219	17997.194230	29.671092
379.574291	18033.924334	29.676109
380.309442	18059.347293	29.681127
380.421093	18085.543184	29.686144
380.566004	18111.858143	29.691162
381.277983	18136.109188	29.696180
381.473403	18164.384590	29.701197
381.934788	18200.987458	29.706215
382.037644	18218.451126	29.711232
382.495928	18255.437651	29.716250
382.846867	18275.234207	29.721268
383.085530	18311.205787	29.726285
383.703300	18340.420514	29.731303
383.923516	18372.213503	29.736320
383.960173	18396.945333	29.741338
384.571035	18434.712517	29.746356
384.596589	18468.434079	29.751373
385.533417	18506.595236	29.756391
385.473579	18542.452699	29.761408
385.814750	18570.983717	29.766426
386.225451	18615.340066	29.771444
386.553416	18656.210875	29.776461
387.025213	18693.525589	29.781479
387.630444	18739.522565	29.786496
388.198385	18768.648552	29.791514
388.196663	18808.369918	29.796532
388.641525	18840.462445	29.801549
389.608121	18874.001003	29.806567
389.654431	18918.639041	29.811584
390.437119	18937.647852	29.816602
390.822977	18964.351541	29.821620
390.926386	18996.013698	29.826637
391.703588	19010.077054	29.831655
392.072494	19042.007549	29.836672
392.717253	19069.387436	29.841690
392.987030	19093.571070	29.846708
393.515575	19114.474238	29.851725
393.717659	19134.594337	29.856743
393.703055	19155.628267	29.861760
394.389845	19187.118755	29.866778
394.916586	19205.325247	29.871796
394.910071	19229.769102	29.876813
395.599429	19244.107264	29.881831
395.278946	19278.727819	29.886848
395.727265	19305.773262	29.891866
396.479529	19332.714944	29.896884
396.508075	19373.097876	29.901901
396.947928	19400.985063	29.906919
397.370423	19438.547627	29.911936
397.756100	19471.306913	29.916954
398.551415	19506.733568	29.921972
398.404776	19540.452649	29.926989
398.921448	19560.026320	29.932007
399.040042	19601.304490	29.937024
399.699848	19631.187660	29.942042
400.266400	19670.156715	29.947060
400.564751	19703.823110	29.952077
400.917783	19741.131426	29.957095
401.236628	19777.003087	29.962112
401.646593	19807.827960	29.967130
402.144940	19848.629422	29.972148
402.490237	19883.273667	29.977165
403.163313	19924.248228	29.982183
403.305727	19966.212251	29.987200
403.563679	20002.584716	29.992218
404.399209	20030.681891	29.997236
404.765143	20078.192893	30.002253
405.782328	20093.901136	30.007271
405.601263	20132.449337	30.012288
406.259933	20164.893751	30.017306
406.912118	20199.335045	30.022324
406.959693	20233.915699	30.027341
407.292533	20254.835294	30.032359
407.670897	20295.834232	30.037376
407.954088	20327.071963	30.042394
408.476352	20365.078881	30.047412
408.757854	20397.439445	30.052429
409.313323	20431.824681	30.057447
409.540616	20467.821728	30.062464
410.034110	20507.378638	30.067482
411.225547	20536.354286	30.072500
411.128061	20566.572329	30.077517
411.801049	20594.785591	30.082535
411.977139	20631.463019	30.087552
412.175743	20663.128385	30.092570
412.644182	20693.175924	30.097588
412.773066	20738.546138	30.102605
413.556037	20769.925998	30.107623
414.062628	20802.609600	30.112640
413.757119	20846.149057	30.117658
414.376774	20886.116403	30.122676
414.997325	20937.201092	30.127693
415.177787	20966.301929	30.132711
415.601196	21006.710293	30.137728
415.904779	21055.519221	30.142746
416.250882	21090.908372	30.147764
416.628887	21139.678450	30.152781
417.317396	21186.141389	30.157799
417.620855	21214.197606	30.162816
418.063126	21262.812387	30.167834
418.489673	21298.478769	30.172852
418.811222	21352.373032	30.177869
419.674330	21386.452443	30.182887
420.160662	21427.636541	30.187904
420.386071	21465.553113	30.192922
420.841613	21493.433328	30.197940
420.958027	21532.925679	30.202957
421.420210	21555.542395	30.207975
421.826992	21595.746823	30.212992
422.337308	21632.900955	30.218010
422.870828	21671.514382	30.223028
423.327796	21713.233757	30.228045
423.543899	21736.156229	30.233063
424.236814	21773.591093	30.238080
424.789336	21805.808712	30.243098
425.692822	21824.647953	30.248116
426.002076	21866.174543	30.253133
426.552382	21881.132328	30.258151
426.881037	21910.054243	30.263168
427.119980	21940.111977	30.268186
427.595243	21969.320363	30.273204
427.834427	22002.372106	30.278221
428.327691	22033.411203	30.283239
428.873024	22069.507356	30.288256
428.810539	22101.365192	30.293274
429.323990	22137.799420	30.298292
429.572200	22185.482476	30.303309
429.815301	22221.718747	30.308327
430.580348	22261.832482	30.313344
430.716233	22311.651842	30.318362
431.543596	22333.947568	30.323380
431.640590	22390.885720	30.328397
431.893576	22442.691591	30.333415
432.627202	22484.535881	30.338432
432.934038	22525.110634	30.343450
433.520813	22561.601464	30.348468
433.905372	22601.146628	30.353485
434.666439	22637.086961	30.358503
435.183686	22663.002308	30.363520
435.411768	22721.687348	30.368538
436.112795	22754.263807	30.373556
436.413672	22792.683319	30.378573
437.273763	22838.513901	30.383591
437.528005	22854.210464	30.388608
437.727481	22900.755781	30.393626
438.302585	22922.496401	30.398644
438.433211	22969.420645	30.403661
439.290862	23008.410883	30.408679
439.806491	23042.235724	30.413696
440.096534	23075.014711	30.418714
440.496314	23112.469448	30.423732
440.658725	23153.296614	30.428749
441.064464	23197.076261	30.433767
441.538403	23229.793637	30.438784
441.871494	23279.867087	30.443802
442.461685	23325.305252	30.448820
442.958927	23373.732581	30.453837
443.021642	23415.779884	30.458855
443.373549	23461.975186	30.463872
443.505896	23501.184131	30.468890
444.090208	23566.252622	30.473908
444.354143	23613.495631	30.478925
445.110425	23656.761309	30.483943
445.851209	23709.122762	30.488960
445.990413	23750.257938	30.493978
446.921270	23805.844286	30.498996
447.193063	23843.107345	30.504013
447.825133	23888.770314	30.509031
449.196188	23900.128595	30.514048
449.332908	23949.030237	30.519066
449.841536	23984.718711	30.524084
450.351174	24018.078194	30.529101
450.474771	24051.684418	30.534119
451.099647	24065.567506	30.539136
451.356022	24100.613570	30.544154
451.698108	24131.654699	30.549172
452.150130	24164.044803	30.554189
452.329326	24202.966964	30.559207
453.007161	24228.575944	30.564224
452.882812	24272.917399	30.569242
453.345888	24304.076040	30.574260
454.074433	24348.652087	30.579277
454.094297	24385.585826	30.584295
454.994434	24435.174822	30.589312
455.153999	24482.737088	30.594330
455.680540	24522.816758	30.599348
455.906276	24570.395145	30.604365
456.101399	24610.780483	30.609383
456.841906	24660.921592	30.614400
457.119279	24711.025819	30.619418
458.092497	24753.544158	30.624436
458.281685	24804.207238	30.629453
458.821928	24854.408805	30.634471
459.328349	24897.165450	30.639488
459.836910	24938.920542	30.644506
460.120520	24985.022470	30.649524
460.908971	25021.723405	30.654541
460.982797	25072.538796	30.659559
461.879363	25108.085132	30.664576
462.090660	25164.919110	30.669594
462.446046	25211.989041	30.674612
463.040465	25249.058394	30.679629
463.592594	25312.623505	30.684647
464.283970	25349.454720	30.689664
464.576939	25399.140517	30.694682
465.517256	25429.842356	30.699700
465.989829	25467.939958	30.704717
466.705005	25508.709864	30.709735
467.112498	25540.499681	30.714752
467.556138	25582.137767	30.719770
467.981401	25605.399934	30.724788
468.748666	25640.831551	30.729805
468.924946	25674.768163	30.734823
469.612890	25713.953513	30.739840
469.365398	25754.534521	30.744858
470.060486	25806.250830	30.749876
470.555043	25842.407575	30.754893
470.665069	25883.645766	30.759911
471.454493	25938.623796	30.764928
471.417693	25980.810570	30.769946
471.920759	26029.991987	30.774964
472.420817	26085.652227	30.779981
472.393366	26133.984856	30.784999
473.081791	26190.860131	30.790016
473.372938	26242.373243	30.795034
474.042846	26296.441746	30.800052
475.136646	26344.510910	30.805069
475.175924	26404.020462	30.810087
475.914472	26446.228546	30.815104
476.326718	26495.325375	30.820122
476.993717	26551.420039	30.825140
477.864694	26600.441395	30.830157
477.858617	26646.620890	30.835175
478.498373	26686.262727	30.840192
478.751090	26741.477076	30.845210
478.848745	26784.835851	30.850228
479.707502	26835.913196	30.855245
480.238816	26887.281338	30.860263
480.592363	26932.083789	30.865280
480.742647	26983.035733	30.870298
481.161324	27027.367177	30.875316
481.563128	27077.110833	30.880333
482.098912	27137.871952	30.885351
482.466859	27181.335324	30.890368
483.150989	27241.586569	30.895386
483.306949	27282.823689	30.900404
484.146800	27338.750439	30.905421
484.140727	27396.920936	30.910439
484.660185	27451.560450	30.915456
485.033178	27506.423044	30.920474
485.249189	27558.567584	30.925492
485.881004	27626.282208	30.930509
486.555788	27682.801948	30.935527
487.286808	27746.094200	30.940544
487.619015	27798.781728	30.945562
488.245041	27851.928720	30.950580
489.129697	27905.272881	30.955597
489.277960	27975.617401	30.960615
490.019892	28019.677205	30.965632
490.896215	28066.307758	30.970650
491.173653	28111.293028	30.975668
492.295795	28155.627890	30.980685
492.607176	28206.774490	30.985703
493.050944	28242.250729	30.990720
493.566448	28303.085550	30.995738
493.695181	28341.124886	31.000756
494.339146	28398.320784	31.005773
494.446311	28450.164252	31.010791
495.413517	28495.418267	31.015808
495.849422	28548.898476	31.020826
496.274438	28609.761940	31.025844
496.782281	28650.868500	31.030861
496.881694	28712.540010	31.035879
497.579369	28757.804535	31.040896
498.161748	28807.558055	31.045914
498.499945	28871.682693	31.050932
499.350611	28920.303939	31.055949
499.739432	28979.714169	31.060967
500.263659	29028.168826	31.065984
500.849847	29082.405015	31.071002
501.121293	29139.056079	31.076020
501.963851	29178.868890	31.081037
502.394951	29237.099544	31.086055
502.982753	29294.181500	31.091072
503.640306	29339.327992	31.096090
504.226247	29383.719878	31.101108
504.980145	29425.592042	31.106125
505.030192	29474.564752	31.111143
505.369621	29521.808418	31.116160
506.391448	29568.071989	31.121178
506.638225	29618.602514	31.126196
507.404564	29670.918038	31.131213
507.976988	29723.653767	31.136231
508.366445	29765.176851	31.141248
508.753758	29806.110474	31.146266
509.279198	29868.128974	31.151284
510.155278	29896.890399	31.156301
510.462202	29954.686549	31.161319
511.179329	29992.165430	31.166336
511.556293	30032.312633	31.171354
512.246563	30071.455471	31.176372
512.615076	30112.572737	31.181389
512.815933	30167.582610	31.186407
513.367371	30208.310255	31.191424
514.095463	30266.151440	31.196442
513.894525	30314.814642	31.201460
514.480741	30359.167964	31.206477
515.042736	30417.503984	31.211495
515.845797	30465.437076	31.216512
516.385153	30506.249436	31.221530
516.460160	30554.369277	31.226548
517.092738	30589.285979	31.231565
517.610629	30638.468612	31.236583
517.906352	30684.142113	31.241600
518.518391	30736.107755	31.246618
518.586865	30796.208058	31.251636
519.298700	30843.680884	31.256653
519.622059	30902.521698	31.261671
520.077011	30958.605743	31.266688
520.566362	31018.889679	31.271706
520.881766	31079.868227	31.276724
521.557125	31143.106352	31.281741
522.309402	31201.798456	31.286759
522.530308	31261.332541	31.291776
523.315141	31326.540820	31.296794
523.571423	31378.554514	31.301812
524.417353	31441.276534	31.306829
525.290076	31514.127965	31.311847
525.331050	31561.663070	31.316864
526.075720	31610.631148	31.321882
526.432459	31683.076337	31.326900
527.594582	31737.127858	31.331917
527.592705	31805.272625	31.336935
528.387010	31862.729562	31.341952
529.325336	31913.493238	31.346970
529.598847	31975.257949	31.351988
530.473834	32016.403307	31.357005
530.915478	32081.339804	31.362023
531.472683	32133.586829	31.367040
532.125953	32183.322503	31.372058
532.293138	32240.593996	31.377076
532.937146	32295.407999	31.382093
533.248650	32358.656971	31.387111
533.706773	32416.559323	31.392128
534.536509	32474.940007	31.397146
534.571775	32532.571834	31.402164
535.150107	32599.387040	31.407181
535.817925	32656.384732	31.412199
536.672387	32728.840364	31.417216
537.142459	32777.134525	31.422234
537.370719	32841.241403	31.427252
538.493076	32892.141580	31.432269
538.303526	32958.393997	31.437287
539.143683	33031.424323	31.442304
540.054709	33076.286188	31.447322
540.323382	33148.452209	31.452340
541.182890	33194.739578	31.457357
541.304910	33252.775916	31.462375
542.140584	33318.541666	31.467392
542.570584	33376.212016	31.472410
542.982542	33436.100531	31.477428
543.322858	33487.409261	31.482445
544.286518	33563.289536	31.487463
544.515466	33619.170128	31.492480
545.116461	33674.427799	31.497498
545.706234	33734.530914	31.502516
546.884694	33786.604498	31.507533
547.580831	33843.175377	31.512551
548.009776	33888.866750	31.517568
548.796531	33935.357398	31.522586
549.254951	33993.359533	31.527604
549.799517	34035.892598	31.532621
550.402005	34095.480513	31.537639
550.699473	34146.608908	31.542656
551.442566	34182.786127	31.547674
551.714407	34237.702342	31.552692
552.273796	34296.193656	31.557709
552.683579	34349.815801	31.562727
553.103000	34397.797745	31.567744
553.456319	34440.161421	31.572762
553.484492	34499.750888	31.577780
554.332684	34547.608775	31.582797
555.194603	34611.800419	31.587815
555.178981	34677.898000	31.592832
555.839362	34726.292268	31.597850
556.256991	34800.365263	31.602868
556.926403	34854.444618	31.607885
557.649014	34915.138808	31.612903
558.056691	34993.256484	31.617920
558.527774	35052.758870	31.622938
559.044586	35109.388648	31.627956
559.592368	35172.065885	31.632973
560.337738	35239.740713	31.637991
560.666528	35318.655431	31.643008
561.492483	35374.660672	31.648026
562.062868	35445.511329	31.653044
562.716921	35504.656818	31.658061
563.471598	35564.814623	31.663079
564.115694	35629.613932	31.668096
565.023155	35677.215774	31.673114
565.164303	35742.313148	31.678132
565.525910	35799.848032	31.683149
566.435772	35858.226633	31.688167
566.880118	35922.911681	31.693184
567.822955	35982.071013	31.698202
568.009209	36050.046383	31.703220
568.492711	36111.102866	31.708237
568.936445	36178.644885	31.713255
569.847911	36240.385348	31.718272
570.676964	36305.052418	31.723290
571.107300	36364.417582	31.728308
571.588018	36420.906003	31.733325
572.121566	36475.609158	31.738343
572.720363	36551.164809	31.743360
573.284753	36610.196221	31.748378
573.956511	36673.956476	31.753396
574.142064	36745.566971	31.758413
574.930961	36802.453825	31.763431
575.465890	36874.928643	31.768448
575.944391	36943.439810	31.773466
576.186370	37014.543426	31.778484
576.993999	37080.993605	31.783501
577.756152	37149.935253	31.788519
578.022784	37220.341307	31.793536
579.473889	37281.560709	31.798554
579.957815	37358.836630	31.803572
580.259938	37415.966779	31.808589
581.193983	37476.404353	31.813607
581.250162	37541.112004	31.818624
582.090705	37607.826953	31.823642
582.505157	37672.744163	31.828660
583.145067	37742.405750	31.833677
583.874916	37793.757199	31.838695
584.127604	37867.223127	31.843712
584.939679	37919.637566	31.848730
586.039192	37990.455065	31.853748
586.266277	38061.584208	31.858765
586.565788	38114.528879	31.863783
586.982276	38186.943323	31.868800
587.615999	38252.883699	31.873818
588.071468	38330.900702	31.878836
588.859095	38397.501067	31.883853
589.762652	38453.152773	31.888871
590.304877	38514.172994	31.893888
591.179470	38575.788698	31.898906
591.683385	38625.396591	31.903924
592.102778	38685.907439	31.908941
592.795254	38740.168293	31.913959
592.825461	38804.862662	31.918976
593.504707	38858.046629	31.923994
594.122556	38925.671190	31.929012
594.775969	38996.875624	31.934029
595.478738	39055.406124	31.939047
595.642854	39120.328844	31.944064
596.302414	39180.950023	31.949082
596.825438	39253.650982	31.954100
597.238282	39322.346143	31.959117
597.587564	39400.754576	31.964135
598.633243	39468.597723	31.969152
599.044177	39546.917695	31.974170
599.506978	39615.801407	31.979188
600.082524	39698.097099	31.984205
601.137998	39764.730846	31.989223
601.415974	39838.184799	31.994240
602.292359	39914.788156	31.999258
602.999078	39981.313008	32.004276
604.008916	40060.296969	32.009293
604.539219	40125.210140	32.014311
604.772764	40195.563776	32.019328
605.400122	40271.259669	32.024346
606.192464	40349.576914	32.029364
606.312205	40414.205395	32.034381
607.180448	40488.138958	32.039399
607.711432	40570.127139	32.044416
608.275415	40641.336994	32.049434
608.982552	40720.395904	32.054452
609.310306	40806.493810	32.059469
610.116272	40882.288997	32.064487
610.452745	40966.066132	32.069504
610.771959	41043.179760	32.074522
611.450316	41118.959124	32.079540
611.888140	41209.898774	32.084557
612.574458	41300.037083	32.089575
613.306594	41399.518295	32.094592
613.637565	41485.880862	32.099610
614.791849	41567.025586	32.104628
615.168245	41645.559124	32.109645
616.494722	41729.798109	32.114663
616.881078	41823.022134	32.119680
617.533733	41889.120910	32.124698
618.181223	41974.256030	32.129716
618.817856	42054.872836	32.134733
619.870836	42133.962797	32.139751
620.490663	42214.602020	32.144768
620.862658	42286.058316	32.149786
621.706656	42360.672680	32.154804
622.255320	42425.556239	32.159821
623.282814	42499.272730	32.164839
624.047461	42571.186163	32.169856
624.265922	42630.344764	32.174874
624.997131	42710.825704	32.179892
625.471119	42787.535941	32.184909
626.282367	42857.378181	32.189927
627.017519	42934.140602	32.194944
627.615682	42998.658112	32.199962
627.958080	43081.367382	32.204980
628.569396	43156.859988	32.209997
629.319064	43226.214993	32.215015
629.947449	43296.025953	32.220032
630.172979	43367.223335	32.225050
630.821798	43440.980872	32.230068
631.389053	43543.866262	32.235085
632.117190	43608.241308	32.240103
632.475369	43683.386395	32.245120
633.125084	43763.165564	32.250138
633.899292	43820.828134	32.255156
633.921819	43902.949855	32.260173
634.689885	43978.729316	32.265191
635.249055	44065.871318	32.270208
635.987032	44135.376883	32.275226
636.520963	44218.981474	32.280244
636.811636	44310.128022	32.285261
637.996852	44392.858642	32.290279
638.596188	44471.354732	32.295296
639.043473	44560.572858	32.300314
639.531450	44636.969557	32.305332
640.364212	44733.086503	32.310349
640.879682	44821.789461	32.315367
641.816368	44916.722010	32.320384
642.080368	45000.589382	32.325402
643.148176	45071.221633	32.330420
644.098644	45159.702807	32.335437
644.913792	45233.070578	32.340455
645.689996	45322.702151	32.345472
646.109651	45395.535985	32.350490
647.241663	45461.956692	32.355508
647.703896	45554.984870	32.360525
648.284818	45621.891830	32.365543
649.025009	45700.467707	32.370560
649.784936	45769.959956	32.375578
651.165357	45838.077548	32.380596
651.280235	45920.388649	32.385613
652.237629	45981.478726	32.390631
652.528521	46059.855616	32.395648
652.680447	46136.471815	32.400666
654.147895	46214.475065	32.405684
654.807276	46298.005093	32.410701
655.005643	46368.627963	32.415719
655.432446	46444.922163	32.420736
656.102962	46528.561889	32.425754
656.605200	46602.971856	32.430772
656.909253	46688.002140	32.435789
657.584463	46781.673785	32.440807
658.302077	46868.104854	32.445824
658.324976	46964.891164	32.450842
659.186114	47059.322884	32.455860
659.533813	47160.856143	32.460877
660.287767	47257.412702	32.465895
661.134573	47354.841726	32.470912
661.682835	47449.696520	32.475930
662.904547	47537.784134	32.480948
663.375753	47647.238073	32.485965
664.032984	47735.208266	32.490983
664.887493	47825.640909	32.496000
665.320678	47928.979882	32.501018
666.304279	48015.028079	32.506036
666.993726	48111.533341	32.511053
667.590760	48191.131646	32.516071
668.552111	48291.698076	32.521088
668.714426	48383.668722	32.526106
669.827720	48475.176447	32.531124
670.596141	48569.106817	32.536141
670.887263	48662.728056	32.541159
671.876678	48746.425987	32.546176
672.490869	48842.176867	32.551194
673.215674	48919.101315	32.556212
673.771937	49022.558548	32.561229
674.308026	49108.224550	32.566247
675.062934	49201.686583	32.571264
675.691919	49302.906955	32.576282
676.066045	49377.595309	32.581300
676.224190	49474.779469	32.586317
677.411857	49563.220026	32.591335
677.726507	49662.533078	32.596352
678.493571	49750.734477	32.601370
679.511128	49846.477475	32.606388
680.205935	49928.549156	32.611405
681.078476	50019.023997	32.616423
681.641453	50109.152466	32.621440
681.997699	50197.502726	32.626458
683.097690	50289.934074	32.631476
683.384140	50387.793321	32.636493
684.205405	50480.075811	32.641511
684.984955	50571.831899	32.646528
685.619244	50669.082451	32.651546
686.309823	50765.610439	32.656564
686.707794	50855.460160	32.661581
687.401902	50955.617351	32.666599
688.220948	51055.299637	32.671616
688.793232	51161.958821	32.676634
689.438397	51248.680739	32.681652
690.161331	51360.435772	32.686669
690.934545	51459.274972	32.691687
691.755867	51554.897835	32.696704
692.349041	51662.437524	32.701722
693.178432	51762.503930	32.706740
693.820975	51870.845179	32.711757
694.259022	51968.235775	32.716775
695.010856	52066.348861	32.721792
695.595626	52189.043957	32.726810
696.474464	52282.446841	32.731828
697.174069	52390.680510	32.736845
697.570719	52507.404381	32.741863
698.838618	52594.654895	32.746880
699.710953	52708.029176	32.751898
700.214252	52807.965334	32.756916
701.034259	52906.137751	32.761933
702.105425	53006.732897	32.766951
702.545182	53114.703979	32.771968
703.247060	53217.136346	32.776986
703.794154	53306.953890	32.782004
704.565730	53421.195497	32.787021
704.816717	53524.165109	32.792039
705.900169	53628.930915	32.797056
706.473368	53739.915785	32.802074
707.068122	53847.075655	32.807092
707.765658	53955.798517	32.812109
708.335981	54074.676342	32.817127
709.297308	54185.763910	32.822144
709.522191	54294.661479	32.827162
710.671107	54396.716660	32.832180
711.311549	54510.442988	32.837197
711.602224	54628.422710	32.842215
712.703741	54726.393553	32.847232
713.195600	54844.853093	32.852250
714.047886	54962.944254	32.857268
715.202120	55072.210736	32.862285
716.065810	55184.413093	32.867303
716.675138	55287.812977	32.872320
716.715010	55395.452039	32.877338
718.029275	55505.755928	32.882356
718.849952	55608.989923	32.887373
719.784652	55727.204752	32.892391
720.678427	55827.022374	32.897408
721.462969	55930.725247	32.902426
722.239951	56021.218603	32.907444
722.941835	56114.814380	32.912461
723.529299	56219.025182	32.917479
724.619270	56311.553204	32.922496
725.213096	56401.971145	32.927514
725.992378	56492.213552	32.932532
726.495981	56566.358503	32.937549
726.777877	56672.700900	32.942567
727.676404	56758.173405	32.947584
728.622421	56847.309451	32.952602
729.075703	56950.775424	32.957620
729.726328	57047.593872	32.962637
729.992694	57149.442619	32.967655
731.208019	57237.777727	32.972672
731.684493	57352.413194	32.977690
732.487751	57451.394645	32.982708
733.335336	57554.027778	32.987725
733.904053	57658.672609	32.992743
734.955168	57766.290277	32.997760
735.309331	57877.069268	33.002778
735.863291	57978.293446	33.007796
736.728384	58087.750751	33.012813
737.438627	58197.619680	33.017831
738.401694	58299.144425	33.022848
738.599258	58415.873086	33.027866
739.400513	58529.159997	33.032884
740.395017	58633.215162	33.037901
740.979082	58752.618096	33.042919
741.575704	58863.090806	33.047936
742.360827	58978.575653	33.052954
742.924311	59103.380607	33.057972
743.655607	59229.940640	33.062989
744.595967	59350.229863	33.068007
745.373066	59473.251418	33.073024
746.137420	59592.680144	33.078042
746.652778	59711.600916	33.083060
747.851187	59838.744867	33.088077
748.212452	59959.480941	33.093095
749.066940	60084.155469	33.098112
750.053145	60203.766055	33.103130
750.754261	60321.876143	33.108148
751.788548	60430.977068	33.113165
752.579537	60560.569023	33.118183
753.212742	60674.325539	33.123200
754.028635	60795.996375	33.128218
754.825902	60905.840496	33.133236
755.888164	61022.106567	33.138253
756.698590	61135.419312	33.143271
757.998747	61239.260555	33.148288
758.643504	61340.037993	33.153306
759.558345	61461.001309	33.158324
760.045009	61554.575962	33.163341
760.566084	61680.294997	33.168359
761.762259	61780.705491	33.173376
762.277520	61892.010894	33.178394
762.789033	62007.393968	33.183412
763.510848	62120.752136	33.188429
764.063043	62239.074975	33.193447
764.905278	62348.805731	33.198464
765.637436	62470.702697	33.203482
766.105979	62588.561045	33.208500
766.973886	62697.227639	33.213517
767.923197	62820.841558	33.218535
768.887446	62934.650889	33.223552
769.455275	63053.513105	33.228570
770.118757	63172.783686	33.233588
771.254852	63290.150304	33.238605
771.765998	63408.063232	33.243623
772.217126	63515.324008	33.248640
773.112498	63640.917483	33.253658
774.146464	63755.383532	33.258676
775.155389	63866.940541	33.263693
775.804216	63976.086237	33.268711
776.868108	64090.587141	33.273728
777.629332	64179.754568	33.278746
778.231034	64296.861240	33.283764
778.578364	64390.604641	33.288781
779.326953	64513.029367	33.293799
780.185220	64619.432255	33.298816
780.844988	64737.353559	33.303834
781.574341	64847.438720	33.308852
782.241384	64961.238850	33.313869
782.889627	65094.233314	33.318887
783.544399	65217.019050	33.323904
784.089503	65346.846360	33.328922
784.885203	65468.124858	33.333940
785.577521	65604.547703	33.338957
786.200840	65729.016783	33.343975
787.305446	65861.106419	33.348992
788.060405	65992.698361	33.354010
788.958571	66114.203933	33.359028
790.406110	66233.615625	33.364045
790.885810	66374.440388	33.369063
791.692886	66497.929205	33.374080
792.386583	66628.466969	33.379098
792.831635	66760.740779	33.384116
793.898060	66887.773389	33.389133
794.939473	67022.744517	33.394151
795.658960	67141.314441	33.399168
796.651207	67274.354573	33.404186
797.084677	67414.903204	33.409204
797.911624	67528.368595	33.414221
798.439728	67676.186021	33.419239
799.795354	67793.965528	33.424256
800.654471	67919.451868	33.429274
801.244354	68050.609921	33.434292
802.639238	68180.902520	33.439309
803.339952	68304.735683	33.444327
803.912811	68434.938008	33.449344
804.955860	68569.621710	33.454362
805.910378	68698.858591	33.459380
806.224197	68828.897500	33.464397
807.030259	68963.186627	33.469415
807.933863	69092.175120	33.474432
808.934203	69225.257903	33.479450
809.398235	69372.933464	33.484468
810.575836	69491.491599	33.489485
811.312686	69631.954380	33.494503
812.069071	69759.011317	33.499520
813.385411	69888.575088	33.504538
814.158373	70015.055482	33.509556
814.819012	70140.227444	33.514573
815.450304	70270.602151	33.519591
816.540910	70399.548775	33.524608
817.141207	70526.408473	33.529626
817.639615	70660.670662	33.534644
818.966755	70790.453133	33.539661
819.618691	70916.023114	33.544679
820.347486	71053.853721	33.549696
821.458157	71175.214363	33.554714
822.331523	71306.554458	33.559732
823.088347	71432.793037	33.564749
823.735583	71568.237724	33.569767
824.601124	71692.619903	33.574784
825.957058	71796.580626	33.579802
826.771075	71932.847370	33.584820
827.514503	72048.241406	33.589837
828.566047	72172.469201	33.594855
829.318533	72289.620875	33.599872
830.207920	72415.350155	33.604890
830.734106	72535.727441	33.609908
831.407223	72643.472511	33.614925
831.800783	72767.799756	33.619943
832.481738	72886.199543	33.624960
833.618842	73015.976320	33.629978
834.161695	73141.014582	33.634996
834.843589	73261.054043	33.640013
835.915960	73407.423996	33.645031
836.100348	73533.067542	33.650048
837.067414	73664.596305	33.655066
837.910322	73801.268504	33.660084
838.690215	73949.265004	33.665101
839.425848	74089.466371	33.670119
840.157625	74219.165542	33.675136
841.024555	74364.753811	33.680154
841.721975	74517.586536	33.685172
843.047066	74654.962332	33.690189
843.544504	74797.730831	33.695207
844.359117	74951.040519	33.700224
845.096943	75100.228069	33.705242
845.874956	75249.770476	33.710260
846.852517	75403.650903	33.715277
847.652007	75560.104120	33.720295
848.665842	75707.055773	33.725312
849.855839	75846.655883	33.730330
850.844489	75997.401853	33.735348
851.991930	76127.840612	33.740365
852.936642	76283.136650	33.745383
853.401487	76425.965445	33.750400
854.433020	76562.914751	33.755418
854.975423	76718.659765	33.760436
855.825352	76858.398367	33.765453
856.820575	77009.909150	33.770471
857.384075	77155.667312	33.775488
858.493290	77313.719966	33.780506
858.945155	77486.264629	33.785524
860.026283	77626.608722	33.790541
861.063521	77789.616282	33.795559
861.576613	77937.304334	33.800576
862.385377	78092.338311	33.805594
863.182137	78255.306786	33.810612
864.605229	78400.886951	33.815629
865.717613	78547.727448	33.820647
866.221098	78703.505529	33.825664
867.754104	78856.312699	33.830682
868.327486	79013.782859	33.835700
869.521423	79148.052168	33.840717
870.642413	79301.069579	33.845735
871.162495	79445.116858	33.850752
872.204973	79585.954119	33.855770
872.907760	79729.928791	33.860788
873.972326	79881.251660	33.865805
875.141088	80025.594071	33.870823
875.652588	80163.910254	33.875840
876.964963	80300.804653	33.880858
877.451645	80443.383710	33.885876
878.345908	80594.397938	33.890893
879.257873	80744.815651	33.895911
880.061643	80892.253876	33.900928
880.869296	81036.061478	33.905946
881.647988	81178.217438	33.910964
882.531021	81322.153586	33.915981
883.474444	81466.479208	33.920999
884.068614	81619.890416	33.926016
884.968331	81772.164160	33.931034
885.695853	81930.951453	33.936052
886.888587	82081.926364	33.941069
887.388787	82227.810310	33.946087
888.279174	82384.631802	33.951104
889.412480	82519.045140	33.956122
889.750474	82662.561067	33.961140
890.473173	82807.526338	33.966157
891.608346	82960.945860	33.971175
892.485695	83116.793991	33.976192
893.501371	83274.657423	33.981210
894.341156	83414.716984	33.986228
895.072952	83574.078096	33.991245
895.963706	83719.590796	33.996263
896.320722	83877.769597	34.001280
897.663135	84032.130055	34.006298
898.649708	84194.294032	34.011316
899.757225	84339.838150	34.016333
900.784324	84491.615570	34.021351
901.084754	84665.391699	34.026368
902.619991	84822.496736	34.031386
903.703293	84977.431457	34.036404
904.563035	85140.103887	34.041421
905.158299	85293.039784	34.046439
905.985209	85459.604589	34.051456
906.954282	85629.285296	34.056474
907.741891	85782.123076	34.061492
908.606590	85942.453018	34.066509
909.651974	86105.272422	34.071527
910.429176	86282.480880	34.076544
911.262377	86447.419349	34.081562
912.002988	86625.313473	34.086580
912.978562	86794.830802	34.091597
914.036626	86959.014463	34.096615
914.914325	87129.297012	34.101632
915.771248	87298.508573	34.106650
916.689748	87472.342898	34.111668
917.676151	87644.104536	34.116685
918.685336	87816.882411	34.121703
919.603678	87997.801208	34.126720
920.949631	88169.171970	34.131738
922.067652	88333.538888	34.136756
923.263518	88498.659760	34.141773
924.524013	88645.907783	34.146791
925.581102	88819.153384	34.151808
926.617538	88963.637161	34.156826
927.654671	89124.156632	34.161844
928.158568	89281.911329	34.166861
929.176548	89432.893509	34.171879
929.808370	89606.949157	34.176896
930.575053	89755.836011	34.181914
931.590545	89928.818185	34.186932
932.187626	90095.700735	34.191949
933.058799	90260.001589	34.196967
933.432382	90440.718976	34.201984
934.759443	90613.395236	34.207002
935.713456	90783.413148	34.212020
936.749766	90952.899757	34.217037
937.587496	91128.856386	34.222055
938.421191	91309.649945	34.227072
939.553032	91483.358309	34.232090
940.559878	91651.892804	34.237108
941.314371	91838.266258	34.242125
942.540231	92004.779884	34.247143
943.093041	92182.911405	34.252160
944.137249	92347.248672	34.257178
945.138849	92535.491695	34.262196
945.762622	92708.381459	34.267213
946.912992	92889.875109	34.272231
947.690833	93067.393756	34.277248
948.793957	93243.897992	34.282266
949.528607	93424.793423	34.287284
950.362533	93599.813072	34.292301
951.389033	93776.061687	34.297319
952.234115	93945.904754	34.302336
953.180512	94121.384283	34.307354
953.974715	94293.257202	34.312372
954.462957	94476.568298	34.317389
955.483379	94644.425201	34.322407
956.831085	94826.312164	34.327424
957.274757	95018.856649	34.332442
958.502359	95206.677993	34.337460
959.496687	95395.425431	34.342477
960.896135	95561.618345	34.347495
961.716910	95753.296150	34.352512
962.744447	95937.402640	34.357530
963.522322	96125.995211	34.362548
964.494636	96313.658293	34.367565
965.830199	96487.678987	34.372583
966.480244	96673.771247	34.377600
967.398755	96856.510027	34.382618
969.039307	97057.791744	34.387636
969.781876	97233.833583	34.392653
971.153937	97412.146522	34.397671
971.994669	97597.986361	34.402688
973.194836	97775.260497	34.407706
974.246361	97961.011277	34.412724
974.898423	98132.396394	34.417741
976.099769	98314.339578	34.422759
976.672348	98504.927544	34.427776
977.403072	98693.844949	34.432794
978.705539	98890.911634	34.437812
979.518226	99079.603182	34.442829
980.291080	99267.764629	34.447847
981.032314	99471.031181	34.452864
982.132812	99653.507190	34.457882
983.298652	99866.715588	34.462900
984.165390	100065.971551	34.467917
985.573173	100257.435182	34.472935
986.185963	100467.549243	34.477952
986.710302	100672.811187	34.482970
987.530787	100875.031361	34.487988
988.637531	101088.956226	34.493005
989.896428	101301.971424	34.498023
990.873180	101510.223346	34.503040
991.850239	101717.539908	34.508058
993.542349	101909.475556	34.513076
994.285608	102127.995974	34.518093
995.614339	102312.941623	34.523111
996.340243	102508.916051	34.528128
997.471836	102709.124024	34.533146
998.897734	102909.842138	34.538164
999.399809	103111.929989	34.543181
1000.675323	103303.121763	34.548199
1001.869615	103499.608920	34.553216
1002.829753	103700.986274	34.558234
1003.792692	103888.903549	34.563252
1004.853753	104091.761567	34.568269
1006.002099	104282.253436	34.573287
1007.248853	104483.247643	34.578304
1007.972169	104678.023262	34.583322
1008.978259	104869.777647	34.588340
1009.680883	105065.186443	34.593357
1011.104363	105269.108251	34.598375
1011.874623	105462.754886	34.603392
1012.745967	105655.385792	34.608410
1013.850928	105841.900665	34.613428
1014.459677	106060.666457	34.618445
1015.411184	106252.946583	34.623463
1016.700090	106453.911010	34.628480
1017.531817	106660.233644	34.633498
1018.715881	106856.545170	34.638516
1019.336907	107049.442928	34.643533
1020.321652	107240.040339	34.648551
1021.371852	107436.593584	34.653568
1022.523209	107632.435001	34.658586
1023.359107	107833.054101	34.663604
1024.139408	108036.229640	34.668621
1024.863786	108238.922009	34.673639
1025.972321	108451.140350	34.678656
1026.572203	108655.984265	34.683674
1027.851106	108864.555384	34.688692
1029.086287	109082.812087	34.693709
1030.107508	109288.946544	34.698727
1031.675834	109495.600237	34.703744
1032.468485	109708.944661	34.708762
1033.837803	109919.434327	34.713780
1034.964590	110127.698398	34.718797
1035.910695	110332.548625	34.723815
1037.610326	110529.422733	34.728832
1038.345972	110745.647421	34.733850
1039.505718	110934.924945	34.738868
1040.399085	111138.751312	34.743885
1041.342737	111354.997189	34.748903
1042.301260	111564.934138	34.753920
1043.319850	111780.335000	34.758938
1044.538541	111985.178045	34.763956
1045.583942	112207.012813	34.768973
1046.379322	112416.907249	34.773991
1047.549988	112637.812776	34.779008
1048.357041	112854.118415	34.784026
1049.623992	113062.711183	34.789044
1050.699150	113277.721790	34.794061
1051.402693	113495.987747	34.799079
1052.988123	113724.586318	34.804096
1053.942736	113947.792943	34.809114
1054.948111	114167.534556	34.814132
1055.982143	114382.636564	34.819149
1056.703656	114610.156242	34.824167
1057.960087	114832.636068	34.829184
1058.962064	115065.117245	34.834202
1060.048987	115284.081436	34.839220
1061.182545	115500.062464	34.844237
1062.661631	115716.418863	34.849255
1064.186722	115925.940721	34.854272
1065.018922	116140.494161	34.859290
1066.243193	116349.764786	34.864308
1067.562167	116562.290024	34.869325
1068.788443	116780.837481	34.874343
1069.737589	116984.076910	34.879360
1070.592131	117206.249165	34.884378
1071.533746	117413.053087	34.889396
1072.573823	117638.365532	34.894413
1073.819135	117846.275431	34.899431
1075.089099	118057.388292	34.904448
1075.736115	118285.000672	34.909466
1077.086439	118484.675000	34.914484
1078.087187	118701.969454	34.919501
1078.683780	118917.621776	34.924519
1080.082312	119130.913329	34.929536
1081.392711	119350.201530	34.934554
1082.490919	119568.145331	34.939572
1083.228678	119783.793524	34.944589
1084.272700	120005.829570	34.949607
1085.263291	120223.580689	34.954624
1085.973456	120450.959061	34.959642
1087.273431	120679.863759	34.964660
1088.055438	120907.664673	34.969677
1089.228555	121130.118850	34.974695
1090.382413	121337.131409	34.979712
1091.165864	121556.029132	34.984730
1092.360137	121770.793082	34.989748
1093.056440	121985.514098	34.994765
1094.465155	122216.503752	34.999783
1095.549739	122440.553829	35.004800
1096.626171	122669.663099	35.009818
1097.875435	122883.627783	35.014836
1099.103429	123105.669729	35.019853
1099.647649	123335.391590	35.024871
1100.926651	123557.327131	35.029888
1102.013603	123788.141444	35.034906
1103.395590	124016.729162	35.039924
1104.462728	124247.727735	35.044941
1105.264523	124470.990807	35.049959
1106.753278	124705.497056	35.054976
1107.578567	124942.319772	35.059994
1109.145536	125170.518282	35.065012
1110.359758	125413.895876	35.070029
1111.117314	125650.849427	35.075047
1111.986360	125879.624776	35.080064
1113.154837	126114.068174	35.085082
1114.248929	126356.129824	35.090100
1115.522920	126605.767928	35.095117
1116.568609	126841.225779	35.100135
1117.634293	127079.318325	35.105152
1118.701366	127332.342468	35.110170
1119.904354	127568.781231	35.115188
1120.904581	127825.153784	35.120205
1121.773381	128078.406952	35.125223
1123.494539	128319.087917	35.130240
1124.339576	128563.565653	35.135258
1125.821162	128817.103994	35.140276
1126.843214	129064.965960	35.145293
1127.872603	129309.672676	35.150311
1129.453867	129562.959867	35.155328
1130.240605	129823.237471	35.160346
1131.277278	130070.838898	35.165364
1132.828464	130323.744332	35.170381
1133.595586	130567.921195	35.175399
1134.875569	130811.077324	35.180416
1136.092788	131071.053448	35.185434
1136.989008	131325.875031	35.190452
1138.099042	131584.301320	35.195469
1139.052256	131844.416152	35.200487
1140.797988	132090.496799	35.205504
1141.513526	132357.170519	35.210522
1142.829785	132613.251470	35.215540
1144.034222	132867.806444	35.220557
1144.979442	133127.730311	35.225575
1146.262622	133387.080775	35.230592
1147.362224	133639.745075	35.235610
1148.592436	133898.994347	35.240628
1149.643702	134158.186517	35.245645
1150.720238	134415.082094	35.250663
1151.772790	134671.147000	35.255680
1152.945493	134937.842837	35.260698
1153.878598	135200.156092	35.265716
1155.648750	135470.548171	35.270733
1156.811372	135734.336455	35.275751
1158.223668	135982.783951	35.280768
1159.409978	136243.643954	35.285786
1160.388379	136499.317156	35.290804
1162.047271	136755.044838	35.295821
1162.914831	137015.646662	35.300839
1164.033982	137252.628001	35.305856
1165.328401	137505.176123	35.310874
1166.206895	137741.452693	35.315892
1167.584946	137979.600938	35.320909
1168.423596	138216.914415	35.325927
1169.738048	138447.685053	35.330944
1171.163648	138689.583356	35.335962
1172.220883	138942.244964	35.340980
1173.090362	139185.341697	35.345997
1173.805135	139436.985881	35.351015
1174.907596	139678.424846	35.356032
1176.231232	139937.059773	35.361050
1177.351010	140186.347816	35.366068
1178.675999	140443.528310	35.371085
1179.412229	140712.751819	35.376103
1180.971809	140966.347364	35.381120
1182.278807	141231.803759	35.386138
1183.187804	141485.890951	35.391156
1184.423521	141756.079991	35.396173
1185.607902	142027.433498	35.401191
1187.004032	142289.244304	35.406208
1187.967446	142554.273160	35.411226
1189.135423	142824.583234	35.416244
1190.217719	143096.038100	35.421261
1191.282237	143379.582316	35.426279
1192.302336	143650.912314	35.431296
1193.478099	143927.557207	35.436314
1194.867112	144207.098306	35.441332
1196.146454	144491.440355	35.446349
1197.401843	144771.122145	35.451367
1198.665772	145041.978871	35.456384
1199.590320	145339.194025	35.461402
1200.922064	145615.864535	35.466420
1202.326208	145890.508954	35.471437
1203.464243	146191.107261	35.476455
1204.900884	146471.343253	35.481472
1206.200254	146752.555219	35.486490
1207.040813	147029.926524	35.491508
1208.520275	147308.323188	35.496525
1209.850197	147596.562385	35.501543
1211.217065	147874.956660	35.506560
1212.714670	148167.066079	35.511578
1213.820067	148431.684455	35.516596
1215.401299	148702.136108	35.521613
1216.461204	148989.758825	35.526631
1218.065621	149238.904450	35.531648
1219.746783	149519.149131	35.536666
1220.854566	149781.443348	35.541684
1222.220775	150058.066202	35.546701
1223.268744	150327.818896	35.551719
1224.304020	150596.446887	35.556736
1225.504045	150866.115000	35.561754
1226.825464	151138.517250	35.566772
1227.902441	151415.515074	35.571789
1229.223971	151679.829454	35.576807
1230.337477	151961.530765	35.581824
1231.137155	152239.049748	35.586842
1232.695166	152510.826837	35.591860
1233.656857	152798.292411	35.596877
1234.757191	153079.598400	35.601895
1235.670449	153360.277803	35.606912
1236.930808	153647.079023	35.611930
1237.931662	153940.863355	35.616948
1239.223583	154234.437014	35.621965
1239.871758	154534.955932	35.626983
1241.114362	154831.041079	35.632000
1242.363178	155136.615363	35.637018
1243.053874	155442.284189	35.642036
1244.457983	155748.243580	35.647053
1245.652321	156057.576067	35.652071
1246.929298	156348.834307	35.657088
1248.071089	156648.818826	35.662106
1249.467080	156955.905303	35.667124
1250.724216	157249.152365	35.672141
1251.744286	157550.267460	35.677159
1253.179505	157846.673539	35.682176
1254.723606	158144.522675	35.687194
1255.425726	158445.646314	35.692212
1256.935404	158744.216007	35.697229
1258.627623	159053.096565	35.702247
1259.684726	159347.457726	35.707264
1261.423117	159648.191030	35.712282
1262.553321	159947.555400	35.717300
1263.530841	160248.139668	35.722317
1264.866593	160568.457312	35.727335
1266.150221	160869.680703	35.732352
1267.429953	161182.933541	35.737370
1268.404136	161496.708603	35.742388
1269.782572	161805.712661	35.747405
1270.958637	162122.097954	35.752423
1272.239420	162444.075887	35.757440
1273.555427	162746.982318	35.762458
1274.296083	163081.829900	35.767476
1275.871933	163396.953667	35.772493
1277.256348	163730.571052	35.777511
1278.415069	164053.444262	35.782528
1279.842929	164368.777365	35.787546
1281.030051	164714.843221	35.792564
1282.891159	165031.632230	35.797581
1283.746983	165370.348638	35.802599
1284.701511	165702.999435	35.807616
1286.724139	166031.023127	35.812634
1287.716761	166370.574929	35.817652
1288.720653	166696.881341	35.822669
1290.312542	167044.662803	35.827687
1291.780211	167361.724219	35.832704
1292.935773	167701.513293	35.837722
1294.518826	168037.516767	35.842740
1296.012325	168362.815881	35.847757
1297.278619	168692.481672	35.852775
1298.231584	169031.553128	35.857792
1300.285021	169356.158067	35.862810
1301.696795	169690.946171	35.867828
1302.923805	170011.923703	35.872845
1304.114909	170347.006900	35.877863
1305.485741	170667.559319	35.882880
1306.914219	171000.514488	35.887898
1308.133908	171341.982975	35.892916
1309.631120	171662.965681	35.897933
1310.921760	171989.301602	35.902951
1312.146877	172311.386975	35.907968
1313.557081	172633.507498	35.912986
1315.107579	172968.588669	35.918004
1316.421540	173283.344185	35.923021
1318.117425	173600.145310	35.928039
1319.245206	173926.141042	35.933056
1320.383586	174252.733718	35.938074
1321.483639	174573.497518	35.943092
1322.792552	174911.754217	35.948109
1324.113775	175233.348911	35.953127
1325.169299	175569.570892	35.958144
1327.092718	175881.476618	35.963162
1328.216322	176209.937965	35.968180
1329.944465	176542.845027	35.973197
1331.683913	176852.503077	35.978215
1332.777515	177185.836543	35.983232
1334.537325	177483.832381	35.988250
1335.448376	177806.387558	35.993268
1336.913215	178101.732650	35.998285
1337.956760	178400.258368	36.003303
1338.989357	178709.473692	36.008320
1340.009474	179012.664633	36.013338
1341.014666	179328.449718	36.018356
1342.480036	179645.353841	36.023373
1343.260693	179980.382252	36.028391
1344.531344	180293.350133	36.033408
1345.678311	180629.096568	36.038426
1346.828383	180963.169388	36.043444
1348.315215	181300.844067	36.048461
1349.702512	181641.596153	36.053479
1350.375475	181997.698823	36.058496
1352.317765	182330.748634	36.063514
1353.710607	182673.575406	36.068532
1355.138927	183027.643935	36.073549
1356.312591	183367.592194	36.078567
1357.893160	183722.059115	36.083584
1359.256916	184066.181695	36.088602
1360.683058	184416.604435	36.093620
1361.990841	184782.889499	36.098637
1363.296960	185141.142796	36.103655
1364.564022	185494.416617	36.108672
1366.013025	185842.737845	36.113690
1367.122334	186217.531573	36.118708
1368.279166	186585.960764	36.123725
1369.947665	186961.060766	36.128743
1371.221406	187324.499854	36.133760
1372.969896	187677.619411	36.138778
1373.999974	188058.429956	36.143796
1375.639453	188419.137482	36.148813
1377.314118	188787.203809	36.153831
1378.479967	189160.687853	36.158848
1380.349440	189525.032934	36.163866
1381.557136	189889.362609	36.168884
1383.092351	190256.572837	36.173901
1384.886915	190627.296921	36.178919
1386.041780	191008.157286	36.183936
1387.743810	191369.901230	36.188954
1389.400884	191736.008951	36.193972
1391.336225	192062.187382	36.198989
1392.867061	192425.781327	36.204007
1394.530780	192763.573039	36.209024
1395.941988	193118.647539	36.214042
1397.086505	193467.154234	36.219060
1398.230863	193814.748935	36.224077
1399.727748	194155.698846	36.229095
1400.771386	194525.263484	36.234112
1402.221341	194882.182604	36.239130
1403.448532	195240.828976	36.244148
1404.904184	195595.694661	36.249165
1406.799078	195945.589540	36.254183
1407.959186	196309.572362	36.259200
1409.117249	196664.683603	36.264218
1410.567625	197027.937089	36.269236
1411.826314	197388.431272	36.274253
1413.017147	197747.478685	36.279271
1414.265402	198121.385128	36.284288
1415.734277	198483.564613	36.289306
1417.423555	198859.014837	36.294324
1418.500834	199223.002329	36.299341
1420.308136	199585.804889	36.304359
1421.316582	199963.113043	36.309376
1422.547468	200327.093895	36.314394
1423.978990	200701.276625	36.319412
1425.306841	201077.129019	36.324429
1426.854925	201467.712821	36.329447
1427.724430	201832.865906	36.334464
1429.289374	202198.972640	36.339482
1430.847709	202573.995266	36.344500
1431.472966	202940.400608	36.349517
1433.278976	203305.102106	36.354535
1434.556138	203694.117877	36.359552
1436.643044	204059.741819	36.364570
1437.300190	204424.143437	36.369588
1438.775414	204812.269178	36.374605
1440.119782	205192.330666	36.379623
1441.302088	205582.134020	36.384640
1443.137676	205962.943713	36.389658
1444.171574	206363.783959	36.394676
1445.647197	206754.560798	36.399693
1447.684415	207139.076137	36.404711
1449.194989	207527.908514	36.409728
1451.365051	207899.086319	36.414746
1452.870433	208278.666989	36.419764
1454.158519	208673.509614	36.424781
1456.224804	209042.614914	36.429799
1457.242670	209423.894157	36.434816
1459.031646	209805.962205	36.439834
1460.522244	210195.115835	36.444852
1461.378777	210570.167181	36.449869
1462.963164	210970.737032	36.454887
1464.086631	211364.908979	36.459904
1465.673466	211770.650348	36.464922
1466.928572	212171.597794	36.469940
1468.342582	212569.117847	36.474957
1469.729099	212972.967961	36.479975
1470.725382	213394.661832	36.484992
1471.820920	213807.858954	36.490010
1473.563656	214219.884578	36.495028
1474.807901	214666.660931	36.500045
1476.058081	215083.521053	36.505063
1477.098772	215527.643242	36.510080
1478.865924	215952.777686	36.515098
1480.007423	216402.220903	36.520116
1481.742048	216848.927109	36.525133
1483.208592	217278.282432	36.530151
1484.924753	217792.248681	36.535168
1486.749836	218235.340076	36.540186
1488.967039	218661.098282	36.545204
1490.344677	219104.191300	36.550221
1492.152190	219529.868510	36.555239
1493.326047	219966.547919	36.560256
1495.196376	220400.879253	36.565274
1496.642947	220824.767444	36.570292
1498.039527	221264.641284	36.575309
1499.994494	221676.816581	36.580327
1501.372479	222114.030224	36.585344
1502.946096	222534.221597	36.590362
1504.718659	222975.640663	36.595380
1505.635311	223399.194875	36.600397
1507.238347	223833.508274	36.605415
1508.764526	224274.084258	36.610432
1510.237719	224705.298376	36.615450
1511.966732	225135.836934	36.620468
1513.226832	225562.390563	36.625485
1514.841411	225988.633267	36.630503
1516.482216	226427.573019	36.635520
1517.912613	226868.631887	36.640538
1519.846871	227290.711733	36.645556
1520.971281	227731.062224	36.650573
1522.499661	228145.261792	36.655591
1524.100517	228585.968482	36.660608
1525.897717	229011.226378	36.665626
1527.663005	229443.755422	36.670644
1528.855651	229871.986125	36.675661
1530.395118	230284.692112	36.680679
1531.610927	230695.700136	36.685696
1533.055508	231105.909632	36.690714
1534.646852	231509.568157	36.695732
1535.942636	231939.718789	36.700749
1537.344003	232364.595330	36.705767
1538.871097	232788.995160	36.710784
1539.941249	233212.125366	36.715802
1541.676499	233641.395685	36.720820
1543.134992	234079.146061	36.725837
1544.967578	234504.135363	36.730855
1546.243308	234954.923776	36.735872
1547.788253	235400.385570	36.740890
1549.203194	235831.340445	36.745908
1550.456440	236275.912911	36.750925
1551.965199	236734.389835	36.755943
1553.630646	237187.177580	36.760960
1554.561737	237653.702968	36.765978
1556.629801	238099.060147	36.770996
1558.193607	238565.788327	36.776013
1560.309233	239030.394485	36.781031
1561.959250	239481.920422	36.786048
1563.260127	239943.310188	36.791066
1565.291714	240396.553421	36.796084
1566.829499	240868.219463	36.801101
1568.588690	241314.955945	36.806119
1570.781220	241763.273014	36.811136
1572.826659	242208.008164	36.816154
1574.410194	242648.044791	36.821172
1575.558012	243095.038203	36.826189
1577.435647	243533.427653	36.831207
1579.217488	243978.489155	36.836224
1580.986408	244431.326760	36.841242
1582.813419	244859.540540	36.846260
1584.355778	245304.745515	36.851277
1585.530123	245746.684215	36.856295
1587.539012	246186.910963	36.861312
1588.668899	246630.153939	36.866330
1590.466413	247077.377271	36.871348
1591.512488	247544.158378	36.876365
1593.134586	247989.049529	36.881383
1594.686971	248440.786162	36.886400
1596.119303	248900.672135	36.891418
1597.857066	249354.335414	36.896436
1599.501702	249826.228540	36.901453
1600.728226	250292.932828	36.906471
1602.676599	250738.891327	36.911488
1603.793834	251223.727067	36.916506
1605.336464	251680.702215	36.921524
1606.867508	252154.776008	36.926541
1608.534413	252627.354473	36.931559
1610.387307	253102.646229	36.936576
1611.621430	253572.197772	36.941594
1613.681123	254064.425532	36.946612
1615.018869	254545.341364	36.951629
1616.527956	255013.730894	36.956647
1618.053784	255500.763932	36.961664
1619.428121	255984.087989	36.966682
1621.215571	256463.406648	36.971700
1622.615658	256946.472930	36.976717
1624.313050	257445.443628	36.981735
1626.109551	257946.735273	36.986752
1627.399518	258437.060226	36.991770
1629.294977	258919.588210	36.996788
1630.504638	259429.512592	37.001805
1631.607547	259919.462264	37.006823
1633.729247	260425.578215	37.011840
1635.225026	260923.109522	37.016858
1637.167031	261407.789326	37.021876
1638.523745	261897.138250	37.026893
1639.929943	262370.525665	37.031911
1642.256860	262848.587703	37.036928
1643.629348	263325.155876	37.041946
1645.469468	263804.288689	37.046964
1647.091389	264292.500889	37.051981
1648.800909	264766.091553	37.056999
1650.561859	265242.036007	37.062016
1651.748451	265728.642715	37.067034
1653.724371	266205.668903	37.072052
1655.836589	266698.219051	37.077069
1657.597634	267191.868311	37.082087
1659.633424	267673.989626	37.087104
1661.193956	268146.103910	37.092122
1663.249084	268621.387782	37.097140
1665.051630	269105.705580	37.102157
1666.399031	269583.874236	37.107175
1668.166326	270044.495829	37.112192
1669.546160	270538.662023	37.117210
1671.543321	271009.482055	37.122228
1672.986863	271513.238871	37.127245
1675.083738	271975.582093	37.132263
1676.572905	272465.612509	37.137280
1678.149899	272955.297506	37.142298
1680.146357	273436.199415	37.147316
1681.892549	273929.716258	37.152333
1683.132288	274430.962086	37.157351
1685.083173	274910.573673	37.162368
1686.483465	275404.043525	37.167386
1688.023205	275910.063772	37.172404
1689.610528	276411.248731	37.177421
1691.088883	276920.376276	37.182439
1692.561220	277422.289492	37.187456
1694.182306	277944.473636	37.192474
1696.424024	278457.460202	37.197492
1697.712498	278967.757836	37.202509
1699.124744	279493.097392	37.207527
1701.001644	280006.547021	37.212544
1702.527461	280529.579104	37.217562
1704.579897	281040.609430	37.222580
1706.777504	281564.213871	37.227597
1708.166608	282088.280520	37.232615
1710.126523	282606.713963	37.237632
1711.263858	283140.700526	37.242650
1713.131416	283659.197044	37.247668
1715.265463	284183.642858	37.252685
1716.755013	284724.043959	37.257703
1718.575419	285251.815050	37.262720
1720.245904	285775.240167	37.267738
1722.079238	286305.139457	37.272756
1723.610148	286835.975919	37.277773
1725.511511	287380.923269	37.282791
1727.073654	287908.270945	37.287808
1728.553474	288452.928369	37.292826
1730.185325	288973.300914	37.297844
1732.157703	289525.264704	37.302861
1733.486079	290074.487718	37.307879
1735.189225	290613.537325	37.312896
1736.978061	291165.474078	37.317914
1738.898023	291711.722655	37.322932
1740.461973	292259.399308	37.327949
1742.301219	292803.472211	37.332967
1744.304155	293350.208180	37.337984
1746.347080	293899.322748	37.343002
1748.309660	294425.588330	37.348020
1750.171027	294959.691413	37.353037
1751.760266	295493.811596	37.358055
1753.640968	296012.438414	37.363072
1755.291927	296528.129085	37.368090
1756.673149	297035.759578	37.373108
1758.596886	297543.349074	37.378125
1760.090234	298082.146373	37.383143
1762.586244	298595.071982	37.388160
1764.148363	299127.985606	37.393178
1765.654567	299627.811423	37.398196
1767.568133	300153.143909	37.403213
1768.534897	300684.141359	37.408231
1770.577392	301198.475152	37.413248
1772.383429	301751.501185	37.418266
1773.808972	302274.591964	37.423284
1775.846361	302823.433968	37.428301
1777.247257	303364.656981	37.433319
1779.090816	303912.178678	37.438336
1780.555814	304471.239252	37.443354
1782.348819	305022.089864	37.448372
1784.284710	305571.465978	37.453389
1785.865367	306155.970469	37.458407
1787.766469	306706.970818	37.463424
1789.613432	307274.078094	37.468442
1791.395028	307832.608501	37.473460
1793.396569	308405.295513	37.478477
1794.952871	308974.699860	37.483495
1797.016092	309551.838680	37.488512
1798.767473	310131.869274	37.493530
1800.260901	310707.849666	37.498548
1802.318883	311272.609699	37.503565
1803.871152	311872.570716	37.508583
1805.531584	312447.596910	37.513600
1807.461196	313052.337193	37.518618
1809.470209	313633.518906	37.523636
1811.245385	314211.916034	37.528653
1813.058525	314810.821024	37.533671
1815.256657	315411.511511	37.538688
1816.968022	316003.034118	37.543706
1818.643234	316596.741795	37.548724
1820.589864	317188.901660	37.553741
1822.824564	317776.159055	37.558759
1824.763538	318361.784472	37.563776
1826.710228	318952.380749	37.568794
1828.389963	319543.625503	37.573812
1830.605719	320126.752822	37.578829
1832.762564	320724.663106	37.583847
1834.777687	321293.263890	37.588864
1836.232285	321888.283490	37.593882
1838.522695	322476.634308	37.598900
1840.669376	323050.733734	37.603917
1842.476476	323637.884322	37.608935
1843.965506	324217.617179	37.613952
1845.969622	324798.478581	37.618970
1847.816666	325386.977679	37.623988
1849.521659	325950.866364	37.629005
1851.008782	326552.134330	37.634023
1852.846580	327125.994045	37.639040
1855.044378	327729.570703	37.644058
1856.775045	328327.759778	37.649076
1858.900313	328897.645449	37.654093
1860.535026	329497.488976	37.659111
1862.410496	330090.355709	37.664128
1864.116515	330680.096292	37.669146
1865.613393	331270.322388	37.674164
1867.474821	331868.200139	37.679181
1868.820441	332476.362424	37.684199
1870.538977	333081.080216	37.689216
1872.539999	333693.640195	37.694234
1874.166363	334301.127195	37.699252
1875.899397	334881.045935	37.704269
1877.915940	335488.937839	37.709287
1879.525124	336073.383070	37.714304
1881.158844	336683.177906	37.719322
1882.732271	337282.085570	37.724340
1884.652253	337886.158597	37.729357
1886.206580	338501.809584	37.734375
1888.136482	339115.665266	37.739392
1890.005349	339727.188452	37.744410
1891.567578	340349.771440	37.749428
1893.765403	340976.658704	37.754445
1895.610800	341616.363980	37.759463
1897.516106	342241.557779	37.764480
1899.168069	342876.126236	37.769498
1901.184307	343515.220627	37.774516
1903.158017	344160.049986	37.779533
1904.856999	344807.987285	37.784551
1906.678594	345464.677510	37.789568
1908.994063	346111.632674	37.794586
1910.877451	346771.391229	37.799604
1913.257309	347416.617535	37.804621
1914.902609	348070.559816	37.809639
1916.987550	348727.643573	37.814656
1919.072414	349377.713459	37.819674
1920.712415	350036.171668	37.824692
1923.045887	350696.180946	37.829709
1924.739512	351360.803380	37.834727
1926.486801	352032.614306	37.839744
1928.806796	352701.173910	37.844762
1930.446616	353373.667477	37.849780
1932.489686	354046.312633	37.854797
1933.993026	354715.483837	37.859815
1936.510515	355391.988557	37.864832
1938.896155	356055.639255	37.869850
1940.499479	356737.627655	37.874868
1942.617405	357402.925484	37.879885
1944.312961	358084.166474	37.884903
1946.467601	358769.329645	37.889920
1948.357192	359452.596888	37.894938
1950.498313	360130.254740	37.899956
1952.617157	360815.161485	37.904973
1954.548562	361496.002773	37.909991
1956.795082	362172.594359	37.915008
1958.710138	362856.992686	37.920026
1960.182148	363543.862529	37.925044
1961.945687	364220.803465	37.930061
1964.062493	364919.263945	37.935079
1965.813133	365606.711427	37.940096
1967.908677	366297.362400	37.945114
1969.686953	367004.542629	37.950132
1971.782585	367705.087234	37.955149
1973.443048	368419.211437	37.960167
1975.429073	369119.925558	37.965184
1977.199588	369825.228076	37.970202
1979.285026	370549.971594	37.975220
1981.285121	371248.081484	37.980237
1983.004761	371976.662139	37.985255
1985.023173	372684.253483	37.990272
1987.015608	373399.520566	37.995290
1988.668324	374137.174557	38.000308
1990.750864	374850.292806	38.005325
1992.576229	375585.073201	38.010343
1994.885908	376309.842052	38.015360
1996.917055	377043.087194	38.020378
1998.835162	377767.662268	38.025396
2001.451872	378496.012478	38.030413
2003.301508	379219.376566	38.035431
2005.601474	379924.189745	38.040448
2007.603024	380616.054008	38.045466
2010.082389	381300.725108	38.050484
2012.298062	381989.685864	38.055501
2014.748778	382664.190923	38.060519
2016.721809	383343.274581	38.065536
2018.890934	384001.012972	38.070554
2021.131024	384672.266368	38.075572
2023.207436	385342.417407	38.080589
2025.076516	386011.371867	38.085607
2026.972603	386683.223784	38.090624
2029.129097	387350.911525	38.095642
2031.034161	388035.182257	38.100660
2032.680411	388718.213400	38.105677
2034.572237	389390.237399	38.110695
2036.418619	390082.535568	38.115712
2038.925589	390783.151303	38.120730
2040.499657	391476.604371	38.125748
2042.813110	392164.976877	38.130765
2044.484552	392859.194151	38.135783
2046.617796	393565.790992	38.140800
2049.044928	394261.981153	38.145818
2050.845079	394980.386884	38.150836
2053.176746	395685.710459	38.155853
2054.959348	396394.124238	38.160871
2056.743019	397115.497921	38.165888
2058.300621	397838.944350	38.170906
2060.437699	398566.180549	38.175924
2062.472112	399294.404134	38.180941
2064.572813	400027.261789	38.185959
2066.340034	400769.253886	38.190976
2068.723527	401527.445341	38.195994
2070.615682	402267.021655	38.201012
2072.485807	403013.601793	38.206029
2074.613652	403757.459247	38.211047
2076.743270	404524.862112	38.216064
2079.124449	405278.697366	38.221082
2080.983816	406045.089853	38.226100
2083.173854	406797.142147	38.231117
2085.662639	407566.277401	38.236135
2087.777981	408320.935634	38.241152
2090.052914	409059.433934	38.246170
2091.959227	409840.356991	38.251188
2094.024548	410601.800763	38.256205
2096.618911	411369.823692	38.261223
2098.250962	412122.758954	38.266240
2100.631039	412880.894593	38.271258
2102.394391	413666.644593	38.276276
2104.383077	414427.460401	38.281293
2106.681640	415203.501882	38.286311
2108.710162	415986.732852	38.291328
2110.623402	416757.852837	38.296346
2112.625112	417554.414022	38.301364
2114.454495	418331.224888	38.306381
2116.690851	419121.798053	38.311399
2118.905278	419908.805018	38.316416
2121.227132	420696.757577	38.321434
2122.579939	421495.253118	38.326452
2125.286964	422294.538265	38.331469
2127.219477	423090.279431	38.336487
2128.687518	423895.491014	38.341504
2131.042773	424707.391793	38.346522
2132.817204	425525.868595	38.351540
2134.735155	426340.952546	38.356557
2137.126056	427151.880644	38.361575
2138.900475	427983.693276	38.366592
2140.994878	428813.095587	38.371610
2142.974095	429643.703455	38.376628
2144.908767	430461.025629	38.381645
2147.539909	431276.838087	38.386663
2148.891098	432088.631843	38.391680
2151.297615	432900.324946	38.396698
2153.247663	433718.645934	38.401716
2155.307010	434541.324096	38.406733
2157.130078	435350.295103	38.411751
2159.158171	436184.055929	38.416768
2161.667412	437006.774909	38.421786
2163.906308	437854.308428	38.426804
2166.006457	438681.893387	38.431821
2168.523754	439521.474612	38.436839
2170.336122	440357.396146	38.441856
2172.415804	441207.512803	38.446874
2174.587480	442045.791888	38.451892
2176.726055	442901.704259	38.456909
2179.272982	443758.325882	38.461927
2181.016503	444623.546888	38.466944
2183.106540	445489.789802	38.471962
2185.232886	446356.296017	38.476980
2187.325564	447233.043054	38.481997
2189.750211	448114.455154	38.487015
2191.772625	448996.150520	38.492032
2194.355175	449881.662853	38.497050
2197.068892	450749.312214	38.502068
2199.443874	451621.685935	38.507085
2201.819489	452501.256174	38.512103
2203.901311	453385.187626	38.517120
2206.432179	454269.816968	38.522138
2208.914347	455132.570244	38.527156
2211.353995	456008.796599	38.532173
2213.834442	456882.551928	38.537191
2215.795482	457763.889955	38.542208
2218.026851	458636.954441	38.547226
2219.943939	459527.577781	38.552244
2221.875685	460422.811004	38.557261
2224.240209	461298.014319	38.562279
2226.283117	462200.177621	38.567296
2228.269124	463097.709555	38.572314
2230.339090	464003.628943	38.577332
2232.321812	464923.067876	38.582349
2234.847629	465824.734590	38.587367
2236.742759	466745.012857	38.592384
2238.576490	467669.806583	38.597402
2240.693779	468600.473082	38.602420
2242.680980	469539.606235	38.607437
2244.964918	470478.493231	38.612455
2247.192141	471430.178284	38.617472
2249.428553	472375.043892	38.622490
2251.796454	473323.529279	38.627508
2254.247662	474268.972713	38.632525
2256.978292	475211.342092	38.637543
2258.941731	476166.925155	38.642560
2261.096008	477110.708627	38.647578
2263.755760	478068.403242	38.652596
2265.958921	479026.022675	38.657613
2268.523615	479980.350919	38.662631
2270.970224	480930.204738	38.667648
2273.473018	481873.636820	38.672666
2276.142821	482824.920816	38.677684
2278.063333	483777.843849	38.682701
2280.740444	484719.988241	38.687719
2282.834256	485667.884902	38.692736
2285.034098	486616.673177	38.697754
2287.180985	487551.586687	38.702772
2289.359307	488505.275842	38.707789
2291.913331	489452.087276	38.712807
2293.986888	490401.854676	38.717824
2295.888807	491349.428503	38.722842
2297.964304	492274.361356	38.727860
2300.455551	493209.926368	38.732877
2302.716237	494135.486466	38.737895
2304.465353	495063.806253	38.742912
2306.646505	495991.853228	38.747930
2308.915620	496929.422387	38.752948
2311.454093	497878.903892	38.757965
2313.805526	498813.429100	38.762983
2315.818566	499765.666259	38.768000
2318.029383	500720.944605	38.773018
2320.456198	501662.512966	38.778036
2322.316405	502636.252609	38.783053
2324.777965	503591.022597	38.788071
2327.232040	504563.844971	38.793088
2329.442874	505543.054900	38.798106
2332.132091	506504.830293	38.803124
2334.183311	507505.079049	38.808141
2336.428627	508485.821437	38.813159
2338.400217	509489.490721	38.818176
2340.767052	510482.747386	38.823194
2342.526670	511476.194026	38.828212
2345.141051	512501.297575	38.833229
2347.714497	513515.504370	38.838247
2349.894491	514540.094467	38.843264
2352.257072	515565.243259	38.848282
2354.731434	516590.105264	38.853300
2356.667566	517634.390753	38.858317
2359.019376	518665.385860	38.863335
2361.501271	519723.248398	38.868352
2363.596129	520766.339955	38.873370
2366.369042	521825.068620	38.878388
2368.474067	522881.063630	38.883405
2371.095340	523930.755002	38.888423
2373.540115	524999.594066	38.893440
2375.700919	526064.375262	38.898458
2378.463698	527118.808791	38.903476
2380.792828	528183.865674	38.908493
2383.344293	529251.982539	38.913511
2385.758135	530335.050497	38.918528
2388.274177	531396.121007	38.923546
2390.849871	532461.938636	38.928564
2393.592294	533534.951097	38.933581
2396.105166	534607.067142	38.938599
2398.648084	535674.871484	38.943616
2401.228774	536730.059000	38.948634
2403.708565	537800.888142	38.953652
2406.316897	538866.181765	38.958669
2408.811270	539934.836890	38.963687
2411.514251	540985.314666	38.968704
2414.347720	542041.579969	38.973722
2416.516167	543090.933861	38.978740
2418.931875	544150.028744	38.983757
2421.211855	545198.151241	38.988775
2423.912382	546262.975465	38.993792
2425.673154	547322.944837	38.998810
2428.245934	548387.125096	39.003828
2430.255888	549458.859247	39.008845
2432.312762	550533.418854	39.013863
2434.708714	551609.346998	39.018880
2436.951203	552699.694665	39.023898
2439.096892	553777.554799	39.028916
2441.603840	554881.357546	39.033933
2443.832802	555963.252716	39.038951
2446.583023	557064.374415	39.043968
2448.647568	558171.348298	39.048986
2451.123719	559269.319104	39.054004
2453.734400	560385.466347	39.059021
2456.217821	561462.705139	39.064039
2458.481586	562558.077993	39.069056
2460.883075	563637.463872	39.074074
2463.577735	564705.110111	39.079092
2465.961970	565776.939251	39.084109
2468.656523	566837.631043	39.089127
2471.157802	567914.537967	39.094144
2473.370194	568998.281899	39.099162
2475.957140	570062.844528	39.104180
2478.381639	571155.710438	39.109197
2480.952349	572238.720436	39.114215
2483.142929	573329.230318	39.119232
2485.575322	574422.517809	39.124250
2487.986459	575503.368732	39.129268
2490.554205	576627.809222	39.134285
2492.832749	577726.456090	39.139303
2495.238262	578840.689636	39.144320
2497.402626	579955.465459	39.149338
2500.413869	581082.191425	39.154356
2502.407575	582219.917234	39.159373
2505.071325	583349.603654	39.164391
2507.517267	584492.261039	39.169408
2509.675643	585637.216030	39.174426
2512.489668	586778.495845	39.179444
2514.691892	587946.942705	39.184461
2517.120180	589099.649003	39.189479
2519.904572	590267.625174	39.194496
2522.260962	591455.857285	39.199514
2524.904664	592621.472280	39.204532
2526.976393	593801.148811	39.209549
2529.667239	594984.965406	39.214567
2532.321506	596176.485378	39.219584
2534.760542	597375.234426	39.224602
2538.066427	598554.884225	39.229620
2540.570609	599754.631574	39.234637
2543.396910	600948.292920	39.239655
2545.878709	602140.636529	39.244672
2548.350054	603347.930110	39.249690
2550.981414	604541.253047	39.254708
2553.448815	605752.100014	39.259725
2555.785586	606944.870951	39.264743
2558.813618	608151.817294	39.269760
2560.833545	609366.708469	39.274778
2563.616453	610564.130329	39.279796
2566.152026	611783.480295	39.284813
2568.703156	613005.446871	39.289831
2571.177916	614233.945553	39.294848
2573.467723	615462.289375	39.299866
2576.293541	616692.759557	39.304884
2578.575171	617916.631952	39.309901
2581.214984	619164.359356	39.314919
2583.622973	620402.034469	39.319936
2586.427927	621650.551633	39.324954
2589.577727	622890.821812	39.329972
2591.895876	624136.634915	39.334989
2594.183757	625376.013281	39.340007
2596.834253	626626.431675	39.345024
2599.079885	627877.121015	39.350042
2602.230484	629124.967459	39.355060
2604.732146	630381.615636	39.360077
2607.076897	631643.884411	39.365095
2609.889276	632904.078016	39.370112
2612.289201	634158.646849	39.375130
2615.176961	635416.230606	39.380148
2618.102239	636683.890344	39.385165
2620.341941	637934.339396	39.390183
2623.437430	639192.432058	39.395200
2625.784550	640463.070025	39.400218
2628.450982	641702.465105	39.405236
2630.866690	642931.624961	39.410253
2633.209587	644166.735006	39.415271
2636.052499	645398.670628	39.420288
2638.258614	646639.588512	39.425306
2640.575879	647874.851287	39.430324
2642.960359	649115.236927	39.435341
2645.582068	650371.432979	39.440359
2648.208711	651626.573797	39.445376
2650.359900	652892.699666	39.450394
2653.174026	654150.083955	39.455412
2655.469535	655433.553171	39.460429
2658.107213	656716.450828	39.465447
2660.524621	658012.966271	39.470464
2662.970698	659304.574347	39.475482
2665.466806	660621.849848	39.480500
2667.896233	661935.124454	39.485517
2670.415157	663254.181255	39.490535
2673.189600	664587.701229	39.495552
2675.297375	665930.603592	39.500570
2678.396865	667277.832947	39.505588
2681.062145	668632.656971	39.510605
2683.971072	669987.845593	39.515623
2686.964787	671338.797888	39.520640
2689.134957	672700.834438	39.525658
2691.936783	674073.560736	39.530676
2694.400632	675456.136674	39.535693
2697.072562	676845.285386	39.540711
2699.979083	678241.744383	39.545728
2702.653085	679632.664519	39.550746
2705.437072	681022.065851	39.555764
2708.265272	682428.640723	39.560781
2710.748524	683831.232308	39.565799
2713.468277	685230.639864	39.570816
2716.034123	686661.791255	39.575834
2719.088094	688079.180856	39.580852
2721.813819	689502.310962	39.585869
2724.224542	690938.025991	39.590887
2727.398588	692362.566740	39.595904
2730.081957	693803.933106	39.600922
2732.707774	695231.978147	39.605940
2735.627638	696668.873346	39.610957
2738.519538	698110.599470	39.615975
2741.338148	699557.011956	39.620992
2743.944918	700988.198250	39.626010
2746.608621	702434.014042	39.631028
2749.440632	703880.405592	39.636045
2751.881706	705340.894049	39.641063
2754.747466	706790.413573	39.646080
2757.745687	708250.369154	39.651098
2760.453215	709710.818664	39.656116
2763.430872	711171.321829	39.661133
2766.339178	712626.635398	39.666151
2769.612161	714071.243737	39.671168
2772.733497	715534.391370	39.676186
2775.917905	716965.255201	39.681204
2778.866553	718404.574365	39.686221
2781.950774	719846.246654	39.691239
2784.924720	721268.743652	39.696256
2787.590320	722707.517936	39.701274
2790.461628	724136.218553	39.706292
2793.305693	725572.538110	39.711309
2795.229908	727008.759315	39.716327
2798.506975	728429.433029	39.721344
2801.539361	729878.363098	39.726362
2803.882765	731300.619244	39.731380
2806.546739	732735.911093	39.736397
2809.361665	734179.665713	39.741415
2812.078401	735600.661984	39.746432
2814.797585	737016.914549	39.751450
2817.416185	738424.739899	39.756468
2819.808820	739823.125861	39.761485
2822.428799	741232.134242	39.766503
2825.262704	742649.540631	39.771520
2827.703031	744075.489058	39.776538
2830.400886	745506.463827	39.781556
2833.184179	746929.570810	39.786573
2835.837885	748382.168462	39.791591
2838.491497	749818.279714	39.796608
2841.050318	751277.599628	39.801626
2843.853777	752732.121203	39.806644
2846.637666	754199.673420	39.811661
2849.527798	755676.582399	39.816679
2851.801859	757149.665025	39.821696
2854.508983	758662.370863	39.826714
2857.651346	760156.049233	39.831732
2860.652432	761666.387238	39.836749
2863.311804	763189.076890	39.841767
2865.981312	764690.501015	39.846784
2869.059478	766228.004111	39.851802
2871.670965	767762.810184	39.856820
2874.718494	769299.048307	39.861837
2876.862427	770857.237779	39.866855
2879.693562	772419.557255	39.871872
2882.515156	773993.684146	39.876890
2884.897997	775557.329550	39.881908
2887.487169	777148.651053	39.886925
2890.345532	778763.248933	39.891943
2893.208217	780364.430460	39.896960
2895.807268	781983.510980	39.901978
2898.638141	783605.822187	39.906996
2901.698797	785237.885437	39.912013
2904.921773	786871.611152	39.917031
2907.384018	788516.269333	39.922048
2910.250938	790169.747094	39.927066
2912.795400	791832.058544	39.932084
2916.693671	793484.593596	39.937101
2919.314852	795144.496239	39.942119
2922.587902	796814.625556	39.947136
2925.828794	798486.173597	39.952154
2928.858172	800145.019663	39.957172
2932.203012	801809.193129	39.962189
2934.626349	803480.164597	39.967207
2937.647995	805141.680886	39.972224
2940.896881	806823.250204	39.977242
2943.717510	808485.017323	39.982260
2946.644766	810168.359647	39.987277
2950.085483	811836.490772	39.992295
2953.123445	813502.225631	39.997312
2956.241821	815181.164583	40.002330
2959.013444	816848.558737	40.007348
2962.301740	818526.486959	40.012365
2965.025691	820198.083158	40.017383
2968.090549	821880.280544	40.022400
2970.875769	823562.341357	40.027418
2973.768470	825256.588558	40.032436
2976.985895	826929.428357	40.037453
2979.793768	828623.699431	40.042471
2982.979481	830304.213395	40.047488
2986.227482	831983.163071	40.052506
2989.263947	833649.146311	40.057524
2991.883678	835337.949169	40.062541
2995.113251	837021.486843	40.067559
2997.813050	838701.068939	40.072576
3000.610075	840381.410892	40.077594
3003.413252	842084.416122	40.082612
3006.128904	843754.298225	40.087629
3009.259522	845410.203985	40.092647
3012.280470	847071.429173	40.097664
3015.062272	848719.814877	40.102682
3017.928365	850372.320064	40.107700
3021.004132	852029.890578	40.112717
3023.414014	853697.035040	40.117735
3026.836977	855368.710337	40.122752
3029.581555	857042.860262	40.127770
3032.206154	858724.240857	40.132788
3035.561945	860403.779669	40.137805
3038.818204	862106.440071	40.142823
3041.399232	863786.534320	40.147840
3044.606246	865488.935597	40.152858
3047.909470	867198.594460	40.157876
3051.128510	868907.783000	40.162893
3053.630350	870626.675777	40.167911
3056.590514	872343.838483	40.172928
3059.447118	874077.172097	40.177946
3062.161788	875840.890437	40.182964
3065.067476	877576.871939	40.187981
3068.058211	879346.465189	40.192999
3070.975427	881119.889200	40.198016
3073.929632	882895.960537	40.203034
3076.876371	884683.473809	40.208052
3080.204742	886466.512645	40.213069
3083.088977	888276.112119	40.218087
3086.176621	890080.575608	40.223104
3089.524023	891874.589301	40.228122
3092.713337	893694.499522	40.233140
3095.648785	895502.204747	40.238157
3098.657187	897327.062850	40.243175
3102.119887	899162.728182	40.248192
3105.360885	900987.237724	40.253210
3108.332576	902828.440650	40.258228
3111.587677	904652.049402	40.263245
3114.682785	906489.431244	40.268263
3117.519256	908345.204686	40.273280
3121.431939	910188.351466	40.278298
3124.480060	912034.873464	40.283316
3127.458714	913877.425329	40.288333
3130.610245	915728.651741	40.293351
3133.926537	917575.479844	40.298368
3136.979348	919430.752625	40.303386
3139.692312	921298.502985	40.308404
3143.167621	923159.055682	40.313421
3146.418637	925019.771978	40.318439
3149.359836	926895.621504	40.323456
3152.597056	928758.976474	40.328474
3155.846935	930627.716342	40.333492
3158.703562	932503.528079	40.338509
3162.094014	934374.758779	40.343527
3165.355899	936257.983076	40.348544
3168.746837	938137.259715	40.353562
3171.731582	940023.964945	40.358580
3175.432812	941908.437397	40.363597
3178.761959	943777.952769	40.368615
3181.574391	945660.160967	40.373632
3184.812943	947528.529461	40.378650
3187.550509	949418.931125	40.383668
3190.801640	951296.527189	40.388685
3193.983536	953193.862673	40.393703
3196.637919	955100.621259	40.398720
3200.050930	957056.085951	40.403738
3202.698578	959008.471929	40.408756
3206.347142	960951.234155	40.413773
3209.563712	962909.439555	40.418791
3212.577123	964871.115608	40.423808
3216.071191	966800.304731	40.428826
3219.284098	968733.578748	40.433844
3222.177407	970635.024860	40.438861
3225.339926	972537.455138	40.443879
3228.206135	974447.983016	40.448896
3231.556722	976365.398617	40.453914
3234.642868	978278.121937	40.458932
3237.495585	980200.376708	40.463949
3241.008886	982133.271462	40.468967
3243.782206	984072.838534	40.473984
3246.919358	986012.756732	40.479002
3249.816951	987967.232429	40.484020
3252.996584	989934.607698	40.489037
3256.198911	991906.840858	40.494055
3259.195479	993900.389837	40.499072
3262.470616	995890.958202	40.504090
3265.350731	997893.131197	40.509108
3268.454744	999908.055959	40.514125
3272.109667	1001916.931701	40.519143
3275.304366	1003940.402560	40.524160
3278.562607	1005974.292187	40.529178
3281.955276	1008011.886843	40.534196
3285.188762	1010056.234388	40.539213
3288.285284	1012111.779528	40.544231
3291.207471	1014163.116314	40.549248
3294.349597	1016241.744451	40.554266
3297.643797	1018312.997752	40.559284
3301.236156	1020393.111782	40.564301
3304.598998	1022483.226273	40.569319
3308.148376	1024571.466904	40.574336
3312.067649	1026656.065087	40.579354
3315.224342	1028738.369482	40.584372
3318.397830	1030836.117106	40.589389
3321.915948	1032940.162218	40.594407
3325.157183	1035035.643318	40.599424
3328.572514	1037138.023463	40.604442
3331.600458	1039251.917704	40.609460
3334.880680	1041359.858469	40.614477
3338.295755	1043482.680501	40.619495
3341.721162	1045608.925880	40.624512
3345.045500	1047739.185489	40.629530
3348.336546	1049867.572366	40.634548
3351.568256	1052001.594904	40.639565
3354.922364	1054150.158000	40.644583
3357.337910	1056301.884064	40.649600
3360.793313	1058457.019006	40.654618
3363.584393	1060637.255690	40.659636
3366.763515	1062808.692306	40.664653
3370.144918	1064993.632859	40.669671
3372.864381	1067212.059388	40.674688
3376.499356	1069406.328757	40.679706
3379.877226	1071617.014935	40.684724
3382.693833	1073848.458422	40.689741
3386.237926	1076068.145040	40.694759
3389.255828	1078321.288899	40.699776
3392.829877	1080546.807946	40.704794
3395.870247	1082794.272044	40.709812
3398.632034	1085068.104648	40.714829
3402.031491	1087326.163199	40.719847
3405.613270	1089601.978120	40.724864
3409.221375	1091873.969511	40.729882
3412.478794	1094160.911955	40.734900
3415.825394	1096437.809580	40.739917
3419.331291	1098714.867091	40.744935
3422.732001	1101000.801745	40.749952
3426.167116	1103285.667317	40.754970
3429.600798	1105572.231921	40.759988
3433.248592	1107871.501056	40.765005
3436.765373	1110126.976019	40.770010
3440.213883	1112347.324920	40.775015
3443.551356	1114485.259999	40.780020
3447.265628	1116567.863833	40.785024
3450.389443	1118573.638481	40.790029
3453.707262	1120500.159364	40.795034
3456.837662	1122340.243686	40.800039
3459.960809	1124093.664772	40.805044
3462.801450	1125788.903532	40.810048
3465.391720	1127397.191805	40.815053
3468.075803	1128898.108603	40.820058
3470.451257	1130361.391498	40.825063
3473.042016	1131736.333694	40.830068
3475.457695	1133018.792266	40.835072
3477.400899	1134243.267907	40.840077
3479.804525	1135391.698443	40.845082
3481.597974	1136496.780808	40.850087
3483.780596	1137517.653694	40.855092
3485.678906	1138481.620834	40.860096
3487.100699	1139379.255438	40.865101
3488.851229	1140213.589554	40.870106
3490.453813	1141012.052625	40.875111
3491.925162	1141745.064449	40.880116
3493.682427	1142413.911235	40.885120
3494.814510	1143059.733192	40.890125
3496.627291	1143630.458601	40.895130
3497.335395	1144166.604591	40.900135
3498.757146	1144674.897391	40.905140
3500.127920	1145115.848362	40.910144
3501.048334	1145532.856452	40.915149
3502.281379	1145911.964277	40.920154
3503.247096	1146244.651356	40.925159
3504.185923	1146540.552967	40.930164
3505.369852	1146814.507945	40.935168
3505.757660	1147038.738048	40.940173
3506.419804	1147241.215049	40.945178
3507.130844	1147434.390776	40.950183
3508.027120	1147582.145363	40.955188
3509.130325	1147718.681896	40.960192
3509.470002	1147814.317206	40.965197
3510.131433	1147888.012580	40.970202
3510.564750	1147955.302163	40.975207
3511.184261	1147979.643303	40.980212
3511.576392	1148008.569260	40.985216
3512.049112	1148005.365276	40.990221
3512.767595	1147973.983164	40.995226
3513.121482	1147949.292735	41.000231
3513.583244	1147891.046110	41.005236
3513.838459	1147825.442952	41.010240
3514.192389	1147747.032312	41.015245
3514.741791	1147655.134467	41.020250
3515.096096	1147545.075664	41.025255
3515.690093	1147413.751166	41.030260
3516.158624	1147281.780801	41.035264
3516.143736	1147119.280929	41.040269
3516.491820	1146960.411839	41.045274
3516.533949	1146791.354176	41.050279
3516.760533	1146616.669638	41.055284
3517.395950	1146426.843968	41.060288
3517.533848	1146227.521538	41.065293
3517.625386	1146007.159188	41.070298
3517.813022	1145798.240072	41.075303
3518.025456	1145573.669456	41.080308
3517.885618	1145343.649666	41.085312
3517.899480	1145111.414348	41.090317
3518.739211	1144863.296758	41.095322
3518.635641	1144633.619265	41.100327
3518.743857	1144379.153040	41.105332
3518.948587	1144117.832425	41.110336
3519.190077	1143842.365580	41.115341
3519.210147	1143567.679402	41.120346
3519.171766	1143302.376127	41.125351
3519.203413	1143035.341095	41.130356
3519.356528	1142739.348368	41.135360
3519.252166	1142446.416332	41.140365
3519.547202	1142162.127957	41.145370
3519.621080	1141870.367644	41.150375
3519.709288	1141565.404088	41.155380
3519.793263	1141275.032114	41.160384
3519.446951	1140969.821221	41.165389
3519.556477	1140658.730524	41.170394
3519.608289	1140370.306511	41.175399
3519.693303	1140050.550383	41.180404
3519.755030	1139744.157926	41.185408
3519.730664	1139437.667032	41.190413
3519.658941	1139126.041691	41.195418
3519.711562	1138817.414471	41.200423
3519.630932	1138491.802390	41.205428
3519.833996	1138178.367688	41.210432
3519.681105	1137859.182892	41.215437
3520.199078	1137534.837265	41.220442
3520.246539	1137214.726338	41.225447
3520.003611	1136876.225828	41.230452
3520.309474	1136547.392638	41.235456
3519.970089	1136231.368691	41.240461
3520.421865	1135885.284411	41.245466
3519.981361	1135561.830627	41.250471
3520.108113	1135216.136096	41.255476
3520.199959	1134885.050880	41.260480
3520.257140	1134548.251908	41.265485
3520.239196	1134195.391218	41.270490
3520.435315	1133868.594847	41.275495
3520.325529	1133509.624201	41.280500
3520.506246	1133177.372909	41.285504
3520.242526	1132837.668178	41.290509
3520.383024	1132483.907631	41.295514
3520.300284	1132143.178532	41.300519
3520.450797	1131784.713664	41.305524
3520.255108	1131444.338501	41.310528
3520.316338	1131100.097556	41.315533
3520.478405	1130744.411934	41.320538
3520.184973	1130408.834065	41.325543
3520.614441	1130045.833572	41.330548
3520.229178	1129692.354167	41.335552
3520.278739	1129336.022536	41.340557
3520.069911	1128979.899770	41.345562
3519.915977	1128646.279539	41.350567
3520.099339	1128296.607406	41.355572
3520.336381	1127950.992709	41.360576
3520.107336	1127595.731693	41.365581
3519.944184	1127236.821916	41.370586
3519.771366	1126890.920627	41.375591
3519.680020	1126552.117717	41.380596
3520.166846	1126200.355585	41.385600
3519.751751	1125859.373993	41.390605
3520.122476	1125492.457714	41.395610
3520.148120	1125150.121339	41.400615
3519.995123	1124786.953573	41.405620
3519.998734	1124434.488497	41.410624
3519.722880	1124093.561398	41.415629
3520.219846	1123727.740158	41.420634
3519.617774	1123374.638625	41.425639
3519.818484	1123032.708663	41.430644
3519.990352	1122668.391372	41.435648
3519.518044	1122315.959986	41.440653
3519.931187	1121969.833453	41.445658
3519.798942	1121619.394614	41.450663
3519.603199	1121263.420635	41.455668
3519.751028	1120921.459473	41.460672
3519.573229	1120563.817143	41.465677
3520.163631	1120203.643460	41.470682
3520.021334	1119846.518727	41.475687
3519.996069	1119489.065123	41.480692
3519.653540	1119123.543161	41.485696
3519.562837	1118786.723836	41.490701
3520.026867	1118423.688556	41.495706
3519.773624	1118071.417529	41.500711
3520.297603	1117700.320277	41.505716
3519.779563	1117339.659974	41.510720
3519.646281	1116987.202557	41.515725
3519.623510	1116627.937444	41.520730
3519.692068	1116273.589127	41.525735
3519.620931	1115913.998183	41.530740
3519.589489	1115553.804656	41.535744
3519.465538	1115203.897307	41.540749
3519.412678	1114842.134276	41.545754
3519.381875	1114491.116412	41.550759
3519.564120	1114150.337655	41.555764
3519.326295	1113779.952450	41.560768
3519.035195	1113432.054708	41.565773
3519.486500	1113080.769787	41.570778
3519.404739	1112725.830266	41.575783
3519.445251	1112365.887591	41.580788
3519.669439	1112011.613461	41.585792
3519.390032	1111655.491129	41.590797
3519.713232	1111299.722901	41.595802
3519.215298	1110936.434257	41.600807
3518.879462	1110575.193303	41.605812
3519.224070	1110227.555594	41.610816
3519.297302	1109869.730149	41.615821
3519.054072	1109509.833617	41.620826
3518.998868	1109168.968568	41.625831
3518.787630	1108813.600912	41.630836
3518.536747	1108459.743418	41.635840
3518.386048	1108110.141450	41.640845
3518.789625	1107777.512353	41.645850
3518.697655	1107425.947104	41.650855
3518.489257	1107073.805239	41.655860
3518.398142	1106731.741460	41.660864
3518.612784	1106382.444437	41.665869
3518.872685	1106040.469890	41.670874
3518.594232	1105703.527986	41.675879
3518.546316	1105349.336991	41.680884
3518.545747	1105000.940808	41.685888
3518.317977	1104678.156854	41.690893
3518.527669	1104327.199155	41.695898
3518.399634	1103979.904162	41.700903
3518.386169	1103631.421550	41.705908
3518.508793	1103282.511849	41.710912
3518.042512	1102951.447558	41.715917
3518.317264	1102592.531691	41.720922
3518.413831	1102254.643474	41.725927
3518.216774	1101920.987142	41.730932
3518.371314	1101571.483686	41.735936
3518.195045	1101235.774642	41.740941
3518.274058	1100876.394558	41.745946
3518.296530	1100555.903208	41.750951
3518.082976	1100197.195189	41.755956
3518.034204	1099858.702930	41.760960
3517.695528	1099517.177883	41.765965
3518.178922	1099177.121211	41.770970
3518.008870	1098836.577066	41.775975
3517.757860	1098508.455599	41.780980
3518.098359	1098167.689593	41.785984
3517.897908	1097831.007809	41.790989
3517.725861	1097491.526828	41.795994
3517.836085	1097151.595458	41.800999
3517.784547	1096806.504178	41.806004
3517.850425	1096467.684946	41.811008
3517.419600	1096134.283455	41.816013
3517.799498	1095797.283790	41.821018
3517.625144	1095473.079242	41.826023
3517.427107	1095129.148863	41.831028
3517.482057	1094801.326099	41.836032
3517.007332	1094474.910420	41.841037
3517.300572	1094148.827067	41.846042
3516.931334	1093814.698314	41.851047
3517.235885	1093482.926443	41.856052
3517.113349	1093159.053322	41.861056
3516.995740	1092834.585695	41.866061
3517.232677	1092505.158139	41.871066
3517.106352	1092183.429062	41.876071
3516.913535	1091845.990618	41.881076
3516.995620	1091529.071080	41.886080
3516.797310	1091209.115183	41.891085
3516.822997	1090874.931583	41.896090
3517.172855	1090554.655285	41.901095
3517.374605	1090218.678546	41.906100
3517.256039	1089899.589948	41.911104
3516.856135	1089574.973718	41.916109
3516.802372	1089238.499477	41.921114
3516.623790	1088930.858023	41.926119
3516.849114	1088611.828653	41.931124
3516.917426	1088270.963503	41.936128
3516.442120	1087964.753210	41.941133
3516.803386	1087622.936873	41.946138
3516.581610	1087312.048958	41.951143
3516.616695	1086988.164587	41.956148
3516.552682	1086668.206291	41.961152
3516.243805	1086359.098974	41.966157
3516.213899	1086020.504695	41.971162
3516.315714	1085700.845511	41.976167
3516.286996	1085400.359667	41.981172
3516.342789	1085084.026660	41.986176
3516.188107	1084765.696773	41.991181
3516.246289	1084455.557994	41.996186
3516.146613	1084130.758623	42.001191
3516.301052	1083824.594792	42.006196
3516.546565	1083505.070549	42.011200
3515.952300	1083187.104241	42.016205
3516.312852	1082888.237480	42.021210
3515.984262	1082567.793805	42.026215
3516.082218	1082245.151030	42.031220
3516.030558	1081948.026918	42.036224
3515.981317	1081628.920695	42.041229
3515.663438	1081329.216849	42.046234
3515.289753	1081017.898162	42.051239
3515.680307	1080713.151311	42.056244
3516.192396	1080415.946738	42.061248
3515.704051	1080094.520396	42.066253
3515.650951	1079792.385701	42.071258
3515.847100	1079480.597499	42.076263
3515.834209	1079171.512859	42.081268
3515.718458	1078873.367998	42.086272
3515.481500	1078566.205318	42.091277
3515.865499	1078260.266775	42.096282
3515.649903	1077962.280525	42.101287
3515.548690	1077639.493897	42.106292
3515.778035	1077338.904602	42.111296
3515.311164	1077031.405404	42.116301
3515.308087	1076716.612062	42.121306
3515.178201	1076425.824252	42.126311
3515.160156	1076116.375387	42.131316
3515.233999	1075816.207969	42.136320
3515.198932	1075516.522132	42.141325
3515.480880	1075212.446195	42.146330
3515.259475	1074931.773337	42.151335
3515.096230	1074622.840018	42.156340
3515.236561	1074319.410025	42.161344
3515.104352	1074032.145011	42.166349
3514.965703	1073733.050809	42.171354
3514.938109	1073437.092051	42.176359
3514.716232	1073139.804314	42.181364
3514.710253	1072847.076405	42.186368
3514.523877	1072556.188044	42.191373
3514.944201	1072265.856884	42.196378
3514.696238	1071978.983510	42.201383
3514.546002	1071690.253213	42.206388
3515.072299	1071410.429581	42.211392
3514.644699	1071113.450016	42.216397
3514.890486	1070813.460147	42.221402
3514.750614	1070520.149282	42.226407
3514.464172	1070239.246291	42.231412
3514.565375	1069945.384343	42.236416
3514.414308	1069652.028832	42.241421
3514.886164	1069352.306237	42.246426
3514.566652	1069067.214778	42.251431
3514.240330	1068780.667428	42.256436
3514.423884	1068489.598207	42.261440
3514.003070	1068211.786348	42.266445
3514.171139	1067926.843731	42.271450
3514.140180	1067643.842394	42.276455
3513.995767	1067366.903852	42.281460
3514.038592	1067096.075674	42.286464
3513.758739	1066822.209527	42.291469
3514.137335	1066527.060666	42.296474
3513.955445	1066258.825158	42.301479
3513.899499	1065964.294739	42.306484
3514.035628	1065702.232296	42.311488
3513.963445	1065420.854662	42.316493
3513.986865	1065147.047371	42.321498
3513.931275	1064871.603806	42.326503
3513.910542	1064601.240265	42.331508
3513.658501	1064317.622694	42.336512
3513.801236	1064051.438997	42.341517
3514.041660	1063770.695153	42.346522
3513.645830	1063493.313846	42.351527
3513.443634	1063224.452236	42.356532
3513.803056	1062954.426254	42.361536
3513.472405	1062682.960633	42.366541
3513.844901	1062409.151889	42.371546
3513.642276	1062129.167226	42.376551
3513.477516	1061856.574595	42.381556
3513.385407	1061588.384962	42.386560
3513.287961	1061319.124096	42.391565
3513.496729	1061056.250415	42.396570
3513.603551	1060791.166409	42.401575
3513.586868	1060515.979537	42.406580
3513.918091	1060250.736255	42.411584
3513.475089	1059975.496276	42.416589
3513.235914	1059707.720684	42.421594
3513.414832	1059434.469910	42.426599
3513.662896	1059163.409404	42.431604
3513.415878	1058889.527545	42.436608
3513.028365	1058624.420608	42.441613
3513.008960	1058351.726713	42.446618
3513.059064	1058098.659688	42.451623
3512.894491	1057840.510549	42.456628
3512.879305	1057578.760081	42.461632
3512.726812	1057309.504808	42.466637
3512.786083	1057053.016138	42.471642
3512.763654	1056795.372730	42.476647
3512.897907	1056539.425947	42.481652
3512.916029	1056272.019085	42.486656
3512.508421	1056032.134429	42.491661
3512.861191	1055769.562873	42.496666
3512.740344	1055520.067781	42.501671
3512.614588	1055261.984234	42.506676
3512.787475	1054991.983893	42.511680
3512.509383	1054739.684192	42.516685
3512.649743	1054494.437286	42.521690
3512.944267	1054242.598923	42.526695
3512.707727	1053980.328487	42.531700
3512.551423	1053716.200606	42.536704
3512.496761	1053469.783391	42.541709
3512.758047	1053206.815737	42.546714
3512.419562	1052961.965289	42.551719
3512.260543	1052700.971211	42.556724
3512.237276	1052457.685738	42.561728
3512.202899	1052208.991015	42.566733
3512.418817	1051956.868491	42.571738
3512.417709	1051719.911888	42.576743
3512.344189	1051463.474558	42.581748
3512.445163	1051210.854694	42.586752
3512.107198	1050958.681406	42.591757
3512.174950	1050714.532539	42.596762
3511.992062	1050468.774257	42.601767
3511.858555	1050224.733373	42.606772
3512.132191	1049991.130322	42.611776
3511.834953	1049740.052421	42.616781
3511.874249	1049492.574029	42.621786
3511.902864	1049262.260960	42.626791
3511.746609	1049025.214408	42.631796
3511.884362	1048776.722875	42.636800
3511.762561	1048540.132342	42.641805
3511.938972	1048297.499372	42.646810
3511.992210	1048053.428442	42.651815
3511.574231	1047810.968549	42.656820
3511.688633	1047559.916928	42.661824
3511.270751	1047338.573341	42.666829
3511.738351	1047096.611949	42.671834
3511.542196	1046859.189621	42.676839
3511.423228	1046635.645077	42.681844
3511.649239	1046390.796679	42.686848
3511.434511	1046164.835491	42.691853
3511.259243	1045929.783397	42.696858
3511.408839	1045689.840387	42.701863
3511.074572	1045467.732406	42.706868
3511.706773	1045233.772988	42.711872
3511.456888	1045007.770405	42.716877
3511.287291	1044772.957993	42.721882
3511.355339	1044543.407780	42.726887
3510.950801	1044311.994443	42.731892
3511.192141	1044073.028647	42.736896
3510.812295	1043854.243707	42.741901
3510.910829	1043626.582139	42.746906
3511.063857	1043404.987340	42.751911
3511.154768	1043173.831260	42.756916
3511.070696	1042964.138788	42.761920
3510.889631	1042737.549351	42.766925
3510.917395	1042506.569077	42.771930
3511.122877	1042279.414251	42.776935
3511.049124	1042052.779182	42.781940
3511.231588	1041823.870491	42.786945
3511.035031	1041607.672009	42.791949
3510.920990	1041372.416624	42.796954
3510.655962	1041142.877193	42.801959
3510.455146	1040922.014567	42.806964
3510.436830	1040710.486750	42.811969
3510.338943	1040488.043746	42.816973
3510.526477	1040267.477690	42.821978
3510.343522	1040072.865248	42.826983
3510.507839	1039856.732455	42.831988
3510.640447	1039638.276782	42.836993
3510.129333	1039422.818282	42.841997
3510.356703	1039210.902938	42.847002
3510.492863	1039002.764485	42.852007
3510.296641	1038792.932946	42.857012
3510.530075	1038572.485409	42.862017
3510.406108	1038370.263154	42.867021
3510.590388	1038140.235628	42.872026
3510.345451	1037937.824211	42.877031
3510.143468	1037716.447621	42.882036
3510.589914	1037495.728954	42.887041
3510.525928	1037296.165125	42.892045
3510.365602	1037074.466041	42.897050
3510.580385	1036865.267663	42.902055
3510.124440	1036651.916827	42.907060
3510.318569	1036433.131700	42.912065
3510.307725	1036234.488142	42.917069
3510.159988	1036005.490893	42.922074
3510.363780	1035815.888466	42.927079
3510.117671	1035613.295945	42.932084
3510.090038	1035385.801011	42.937089
3510.047886	1035174.743592	42.942093
3510.008190	1034967.160244	42.947098
3509.646469	1034761.170019	42.952103
3509.668312	1034563.041878	42.957108
3509.879511	1034354.039966	42.962113
3510.126802	1034162.632672	42.967117
3509.582680	1033951.418076	42.972122
3509.795070	1033750.423821	42.977127
3509.706509	1033549.181607	42.982132
3509.345851	1033353.685981	42.987137
3509.500077	1033157.421326	42.992141
3509.602605	1032965.900013	42.997146
3509.620261	1032777.386076	43.002151
3509.685438	1032570.180021	43.007156
3509.849562	1032370.692408	43.012161
3509.490653	1032167.315664	43.017165
3509.523539	1031973.061774	43.022170
3509.516298	1031776.484751	43.027175
3509.237888	1031576.073696	43.032180
3509.266754	1031386.930147	43.037185
3509.127868	1031202.744651	43.042189
3509.548096	1031010.619870	43.047194
3509.322094	1030814.529003	43.052199
3509.225272	1030622.863263	43.057204
3509.689728	1030433.712477	43.062209
3509.442172	1030230.053126	43.067213
3509.469066	1030036.700985	43.072218
3509.519052	1029837.141590	43.077223
3509.280045	1029636.557554	43.082228
3509.292476	1029449.093942	43.087233
3509.271765	1029248.072672	43.092237
3509.336723	1029069.980629	43.097242
3509.466453	1028890.225947	43.102247
3509.244018	1028686.118771	43.107252
3509.277804	1028481.671392	43.112257
3508.918357	1028301.687796	43.117261
3508.965942	1028114.270446	43.122266
3508.959648	1027916.588782	43.127271
3508.869989	1027734.024164	43.132276
3509.025949	1027556.062597	43.137281
3509.100624	1027376.655748	43.142285
3508.628866	1027176.506026	43.147290
3508.832401	1027002.006322	43.152295
3508.791732	1026815.528693	43.157300
3508.632658	1026620.732664	43.162305
3508.339720	1026453.466734	43.167309
3508.422391	1026274.701388	43.172314
3508.386800	1026097.209366	43.177319
3508.406237	1025922.028062	43.182324
3508.519100	1025738.395993	43.187329
3508.421239	1025573.493996	43.192333
3508.428605	1025394.034622	43.197338
3508.380537	1025227.273093	43.202343
3508.365261	1025044.511494	43.207348
3508.594952	1024863.738701	43.212353
3508.387928	1024694.177059	43.217357
3508.459176	1024531.736256	43.222362
3508.671233	1024349.883697	43.227367
3508.129234	1024169.506341	43.232372
3508.295036	1024000.831513	43.237377
3508.147082	1023827.453787	43.242381
3508.171818	1023658.307233	43.247386
3508.143277	1023491.393834	43.252391
3507.814718	1023317.933140	43.257396
3508.052301	1023147.766737	43.262401
3507.901141	1022984.154382	43.267405
3507.780026	1022808.704886	43.272410
3508.480484	1022644.263721	43.277415
3508.010158	1022492.323429	43.282420
3508.005116	1022321.202367	43.287425
3507.929599	1022155.808177	43.292429
3508.187007	1021969.992579	43.297434
3507.872239	1021816.844813	43.302439
3507.967766	1021660.134510	43.307444
3508.212149	1021482.934879	43.312449
3507.897666	1021323.470589	43.317453
3508.092277	1021149.080786	43.322458
3508.147047	1020996.237630	43.327463
3507.885000	1020832.871646	43.332468
3507.891193	1020661.407116	43.337473
3507.924963	1020490.999650	43.342477
3507.693740	1020326.062041	43.347482
3507.830707	1020159.216091	43.352487
3507.584305	1019998.635986	43.357492
3507.975667	1019836.491279	43.362497
3507.726193	1019676.969443	43.367501
3507.577246	1019513.934402	43.372506
3507.743754	1019357.924094	43.377511
3507.889417	1019196.868439	43.382516
3508.102153	1019015.618717	43.387521
3507.881196	1018868.486679	43.392525
3507.841852	1018704.536939	43.397530
3508.057208	1018528.801038	43.402535
3507.625239	1018365.197111	43.407540
3507.669187	1018192.777701	43.412545
3507.614248	1018040.357203	43.417549
3507.127393	1017890.914639	43.422554
3507.319005	1017739.706776	43.427559
3507.586946	1017590.908181	43.432564
3507.340862	1017428.216685	43.437569
3507.217420	1017269.381953	43.442573
3507.152512	1017118.005518	43.447578
3507.324254	1016975.320262	43.452583
3506.918987	1016821.953918	43.457588
3507.104629	1016672.271098	43.462593
3507.361299	1016523.543142	43.467597
3507.208461	1016356.923060	43.472602
3507.151705	1016223.282694	43.477607
3507.094369	1016080.709510	43.482612
3507.056595	1015914.057342	43.487617
3506.962818	1015776.335700	43.492621
3506.635506	1015632.727869	43.497626
3507.053876	1015487.537462	43.502631
3507.012483	1015347.952314	43.507636
3507.071224	1015198.251140	43.512641
3506.960838	1015048.088434	43.517645
3507.141964	1014896.417462	43.522650
3506.973169	1014736.644845	43.527655
3506.756730	1014600.662139	43.532660
3506.660787	1014461.646497	43.537665
3506.788675	1014341.911983	43.542669
3506.908232	1014187.707635	43.547674
3506.978852	1014048.460157	43.552679
3506.856735	1013909.532277	43.557684
3506.977951	1013747.256285	43.562689
3507.091762	1013609.932894	43.567693
3506.618033	1013466.779363	43.572698
3506.642289	1013326.162137	43.577703
3506.347072	1013188.216049	43.582708
3506.418220	1013054.382169	43.587713
3506.475725	1012929.773460	43.592717
3506.476037	1012783.902317	43.597722
3506.813711	1012640.302754	43.602727
3506.315047	1012503.538847	43.607732
3506.330719	1012361.539194	43.612737
3506.399942	1012244.683513	43.617741
3506.569317	1012117.027399	43.622746
3506.316482	1011967.194419	43.627751
3506.600050	1011839.513207	43.632756
3506.443720	1011691.599710	43.637761
3506.517407	1011559.478360	43.642765
3506.492872	1011432.615793	43.647770
3506.347359	1011293.821466	43.652775
3506.296274	1011159.768388	43.657780
3506.381145	1011023.455284	43.662785
3506.198035	1010901.075746	43.667789
3506.328564	1010771.452496	43.672794
3506.321983	1010625.235097	43.677799
3506.546173	1010505.111631	43.682804
3506.453501	1010363.759557	43.687809
3506.103002	1010240.907438	43.692813
3506.014405	1010108.098632	43.697818
3506.206357	1009971.742448	43.702823
3506.113183	1009851.754495	43.707828
3506.227902	1009711.420766	43.712833
3506.257234	1009595.488417	43.717837
3505.886628	1009475.635323	43.722842
3505.923740	1009340.066773	43.727847
3505.825040	1009221.912716	43.732852
3506.353058	1009090.436083	43.737857
3505.996674	1008958.518939	43.742861
3506.195390	1008834.476656	43.747866
3506.184480	1008687.626574	43.752871
3505.908330	1008582.608976	43.757876
3505.934530	1008449.839380	43.762881
3505.800520	1008340.711712	43.767885
3505.984974	1008209.173933	43.772890
3505.841017	1008075.548767	43.777895
3505.589669	1007965.655562	43.782900
3506.083407	1007834.446918	43.787905
3506.171413	1007718.563519	43.792909
3505.915920	1007586.500443	43.797914
3506.207048	1007466.981691	43.802919
3505.957732	1007352.701711	43.807924
3506.019660	1007210.272963	43.812929
3506.047877	1007082.623272	43.817933
3505.870930	1006962.684846	43.822938
3506.329487	1006825.917033	43.827943
3506.149656	1006721.140568	43.832948
3506.157439	1006582.593852	43.837953
3506.074652	1006465.837822	43.842957
3505.925040	1006345.687324	43.847962
3506.333021	1006203.467866	43.852967
3505.985341	1006086.164215	43.857972
3506.157473	1005960.215665	43.862977
3505.800035	1005816.167780	43.867981
3505.698887	1005706.303061	43.872986
3505.570504	1005589.633659	43.877991
3505.438507	1005470.920288	43.882996
3505.936465	1005354.240110	43.888001
3505.733200	1005228.726064	43.893005
3505.481130	1005106.523824	43.898010
3505.637628	1004988.239050	43.903015
3505.433524	1004881.001079	43.908020
3505.746517	1004762.685808	43.913025
3505.863769	1004646.637271	43.918029
3505.706965	1004536.078135	43.923034
3505.512426	1004416.963864	43.928039
3505.738416	1004294.762586	43.933044
3505.523034	1004165.044472	43.938049
3505.783160	1004059.465267	43.943053
3505.346038	1003933.474603	43.948058
3505.722834	1003820.187231	43.953063
3505.647856	1003722.341547	43.958068
3505.470970	1003592.506673	43.963073
3505.501441	1003479.755910	43.968077
3505.323451	1003360.422078	43.973082
3505.664180	1003242.264982	43.978087
3505.256648	1003144.366780	43.983092
3505.271993	1003015.946280	43.988097
3505.474572	1002907.630991	43.993101
3505.189764	1002811.166145	43.998106
3505.545454	1002688.325035	44.003111
3505.326967	1002578.029624	44.008116
3505.295485	1002465.949913	44.013121
3505.255854	1002343.652915	44.018125
3505.406444	1002247.398635	44.023130
3504.964775	1002128.957942	44.028135
3504.659046	1002021.682434	44.033140
3505.071543	1001928.201423	44.038145
3505.056725	1001826.518067	44.043149
3504.947098	1001715.117503	44.048154
3505.514053	1001604.089871	44.053159
3504.969640	1001500.055072	44.058164
3505.173537	1001384.509183	44.063169
3505.112374	1001277.179272	44.068173
3505.162937	1001174.208295	44.073178
3505.311725	1001053.214835	44.078183
3504.705254	1000967.671498	44.083188
3505.129572	1000854.316908	44.088193
3505.044487	1000760.995904	44.093197
3504.637102	1000651.764623	44.098202
3504.821232	1000539.027251	44.103207
3504.741295	1000447.062846	44.108212
3504.769200	1000334.931131	44.113217
3505.000364	1000238.240072	44.118221
3504.591723	1000147.590299	44.123226
3504.838210	1000041.743677	44.128231
3504.698216	999955.426823	44.133236
3504.744031	999849.512320	44.138241
3504.992661	999752.518066	44.143245
3504.743656	999651.515603	44.148250
3504.521226	999550.799003	44.153255
3504.746063	999447.670568	44.158260
3504.784091	999341.455799	44.163265
3504.953415	999259.652879	44.168269
3504.812324	999151.127588	44.173274
3504.753519	999060.500135	44.178279
3504.697683	998971.915244	44.183284
3504.877027	998847.462113	44.188289
3504.703793	998767.363614	44.193293
3504.654354	998666.797519	44.198298
3504.767323	998562.795142	44.203303
3504.827577	998474.572810	44.208308
3504.738622	998370.113326	44.213313
3504.771514	998256.965970	44.218317
3504.973249	998162.678571	44.223322
3504.995306	998053.521152	44.228327
3504.533153	997965.474308	44.233332
3504.353212	997866.765620	44.238337
3504.947923	997773.186028	44.243341
3504.380765	997671.908520	44.248346
3504.431647	997567.800730	44.253351
3504.477774	997475.475156	44.258356
3504.508711	997383.929655	44.263361
3504.349508	997296.309433	44.268365
3504.399556	997210.795917	44.273370
3504.287510	997117.127133	44.278375
3504.420747	997022.637277	44.283380
3504.273313	996930.919058	44.288385
3504.276881	996847.160773	44.293389
3504.223727	996750.262234	44.298394
3504.395444	996672.025201	44.303399
3504.661440	996588.609463	44.308404
3504.539802	996478.081798	44.313409
3504.775994	996381.616306	44.318413
3504.157623	996282.075611	44.323418
3504.420913	996191.641432	44.328423
3504.170655	996117.070228	44.333428
3504.128881	996019.280668	44.338433
3504.441509	995927.665262	44.343437
3504.378910	995848.676191	44.348442
3504.735545	995751.206036	44.353447
3504.258156	995657.475897	44.358452
3504.169943	995570.206960	44.363457
3504.366678	995475.973129	44.368461
3504.219518	995392.997532	44.373466
3504.628874	995297.069594	44.378471
3504.180753	995206.736893	44.383476
3504.633885	995124.924990	44.388481
3504.562426	995032.871287	44.393485
3504.160995	994947.008299	44.398490
3504.065840	994869.277495	44.403495
3504.268647	994779.902489	44.408500
3504.042991	994682.120166	44.413505
3504.040862	994603.396089	44.418509
3504.201193	994509.054770	44.423514
3504.003574	994424.709248	44.428519
3504.106659	994348.107878	44.433524
3504.035420	994259.646748	44.438529
3503.999651	994182.189066	44.443533
3503.799264	994090.920832	44.448538
3503.881241	994013.928666	44.453543
3503.960456	993927.386425	44.458548
3504.019728	993840.651259	44.463553
3504.070578	993786.950525	44.468557
3504.126170	993692.710341	44.473562
3503.920343	993595.295816	44.478567
3503.991276	993514.108362	44.483572
3504.090045	993430.966117	44.488577
3503.968635	993357.701741	44.493581
3503.843960	993273.034727	44.498586
3504.109342	993190.543707	44.503591
3503.843961	993110.770270	44.508596
3504.106780	993034.124869	44.513601
3503.961524	992951.210712	44.518605
3503.679906	992874.457905	44.523610
3504.143253	992785.008595	44.528615
3503.986183	992704.626832	44.533620
3503.824325	992620.053672	44.538625
3504.103878	992533.749600	44.543629
3504.030515	992463.877149	44.548634
3504.196126	992372.326068	44.553639
3503.880693	992290.892357	44.558644
3503.850341	992208.825684	44.563649
3503.680629	992138.770156	44.568653
3503.588242	992061.097917	44.573658
3504.024106	991973.394931	44.578663
3503.737996	991898.871657	44.583668
3503.699919	991816.410674	44.588673
3503.992759	991741.692502	44.593677
3503.813849	991659.739849	44.598682
3504.087227	991586.387601	44.603687
3503.854548	991503.174253	44.608692
3503.881737	991429.080641	44.613697
3503.726360	991342.537660	44.618701
3503.536672	991283.783495	44.623706
3503.512758	991195.559307	44.628711
3503.647500	991131.485634	44.633716
3503.368088	991067.089479	44.638721
3503.765121	990982.302395	44.643725
3503.804501	990911.319845	44.648730
3503.639722	990820.383160	44.653735
3503.469689	990747.873106	44.658740
3503.405922	990677.197116	44.663745
3503.685435	990608.608726	44.668749
3503.298228	990542.079359	44.673754
3503.797399	990456.877616	44.678759
3503.459133	990392.386005	44.683764
3503.806392	990327.098215	44.688769
3503.530225	990241.435913	44.693773
3503.590055	990177.071306	44.698778
3503.862152	990088.001115	44.703783
3503.589156	990028.272594	44.708788
3503.461695	989950.772313	44.713793
3503.543402	989878.112192	44.718797
3503.423305	989812.017849	44.723802
3503.884385	989726.323875	44.728807
3503.495020	989652.275717	44.733812
3503.610877	989574.632719	44.738817
3503.649908	989511.044150	44.743821
3503.521692	989437.632822	44.748826
3503.523115	989360.395832	44.753831
3503.486400	989299.743041	44.758836
3503.364198	989218.526034	44.763841
3503.555868	989142.425046	44.768845
3503.488963	989077.483717	44.773850
3503.634854	988995.536682	44.778855
3503.494657	988926.216919	44.783860
3503.338875	988861.872946	44.788865
3503.276176	988789.905427	44.793869
3502.895648	988726.669791	44.798874
3503.739220	988645.773208	44.803879
3503.500250	988591.388377	44.808884
3503.312323	988513.293257	44.813889
3503.487580	988438.843691	44.818893
3503.186176	988368.860922	44.823898
3503.624477	988312.118472	44.828903
3503.447488	988243.284149	44.833908
3503.428530	988167.497445	44.838913
3503.376201	988102.054871	44.843917
3503.461218	988027.322156	44.848922
3503.261754	987956.244527	44.853927
3503.043481	987899.606109	44.858932
3503.401883	987820.045834	44.863937
3503.473965	987754.773874	44.868941
3503.218484	987686.823695	44.873946
3503.427772	987620.649642	44.878951
3503.542264	987548.344587	44.883956
3503.322157	987473.557307	44.888961
3503.428674	987409.739039	44.893965
3503.188651	987348.123378	44.898970
3503.434597	987277.744369	44.903975
3503.317768	987220.106902	44.908980
3503.259377	987153.386157	44.913985
3503.351499	987089.469112	44.918989
3503.515192	987013.246717	44.923994
3503.355354	986951.125741	44.928999
3503.394303	986883.410167	44.934004
3503.410613	986815.990214	44.939009
3503.335681	986752.096899	44.944013
3503.458568	986677.535371	44.949018
3503.431574	986601.826720	44.954023
3503.401619	986542.704547	44.959028
3503.401316	986476.259014	44.964033
3503.211730	986393.158926	44.969037
3503.420679	986338.288494	44.974042
3503.470117	986262.855472	44.979047
3502.769621	986201.791120	44.984052
3502.728742	986147.447878	44.989057
3503.111338	986069.810730	44.994061
3502.774691	986024.784984	44.999066
3502.930483	985945.817393	45.004071
3502.774232	985894.613322	45.009076
3503.049117	985844.801516	45.014081
3503.178874	985776.179586	45.019085
3503.199010	985707.867639	45.024090
3502.924916	985644.580212	45.029095
3502.986327	985584.359602	45.034100
3503.162879	985528.218081	45.039105
3502.826148	985464.353440	45.044109
3502.983223	985399.138082	45.049114
3503.096878	985341.834006	45.054119
3502.811460	985280.008257	45.059124
3502.695253	985229.279571	45.064129
3502.720773	985169.158079	45.069133
3502.550605	985117.461345	45.074138
3502.637787	985056.450155	45.079143
3503.090149	984998.013283	45.084148
3502.892109	984937.535782	45.089153
3502.948310	984886.190059	45.094157
3502.614869	984835.981644	45.099162
3502.837816	984769.381840	45.104167
3502.804615	984723.027010	45.109172
3502.688368	984659.605041	45.114177
3502.816099	984601.900799	45.119181
3502.499034	984555.981779	45.124186
3502.790738	984486.244002	45.129191
3502.753540	984444.963060	45.134196
3502.610330	984391.986423	45.139201
3502.685611	984339.851780	45.144205
3503.043648	984285.034645	45.149210
3503.039909	984225.103237	45.154215
3502.772499	984162.481515	45.159220
3502.641193	984106.181480	45.164225
3502.982886	984055.854994	45.169229
3502.730357	983982.784246	45.174234
3502.803476	983928.693917	45.179239
3502.885086	983890.513078	45.184244
3502.869532	983813.496496	45.189249
3502.933784	983753.548936	45.194253
3502.777347	983707.206145	45.199258
3502.554003	983647.792935	45.204263
3502.802403	983593.963423	45.209268
3502.503045	983534.952041	45.214273
3502.718437	983471.950348	45.219277
3502.659171	983439.256577	45.224282
3502.907150	983388.353902	45.229287
3502.579535	983334.226315	45.234292
3502.608868	983287.947145	45.239297
3502.787335	983225.632199	45.244301
3502.460815	983182.925366	45.249306
3502.599512	983116.124887	45.254311
3502.488974	983072.502992	45.259316
3502.525347	983012.942761	45.264321
3502.489169	982964.230985	45.269325
3502.283157	982916.815987	45.274330
3502.901372	982870.631708	45.279335
3502.683921	982823.217817	45.284340
3502.413138	982754.918408	45.289345
3503.013210	982711.371983	45.294349
3503.041663	982658.253329	45.299354
3502.770518	982598.348873	45.304359
3502.734446	982548.168959	45.309364
3502.572019	982488.343081	45.314369
3502.971886	982430.962625	45.319373
3502.693288	982375.157965	45.324378
3502.630790	982335.916403	45.329383
3502.542309	982283.399373	45.334388
3502.342848	982231.290716	45.339393
3502.468986	982176.979763	45.344397
3502.204437	982127.029067	45.349402
3502.703635	982077.733316	45.354407
3502.634893	982035.854253	45.359412
3502.801794	981985.831260	45.364417
3502.666237	981924.530319	45.369421
3502.538370	981872.504243	45.374426
3502.665731	981815.357789	45.379431
3502.437983	981764.909604	45.384436
3502.502635	981718.416587	45.389441
3502.905581	981664.543436	45.394445
3502.657488	981623.667428	45.399450
3502.443052	981563.840423	45.404455
3502.172807	981520.232964	45.409460
3502.297533	981461.520901	45.414465
3502.294693	981421.481967	45.419469
3502.298793	981378.121210	45.424474
3502.859033	981336.719376	45.429479
3502.680679	981289.579276	45.434484
3502.550546	981228.562948	45.439489
3502.451373	981170.666064	45.444493
3502.270807	981126.552514	45.449498
3502.801778	981076.852251	45.454503
3502.834358	981029.577598	45.459508
3502.403417	980974.077319	45.464513
3502.677857	980926.566647	45.469517
3502.524843	980878.637647	45.474522
3502.706365	980822.156009	45.479527
3502.582217	980777.249121	45.484532
3502.659305	980730.550678	45.489537
3502.900392	980672.104349	45.494541
3502.662958	980605.922482	45.499546
3502.814178	980556.768608	45.504551
3502.936334	980510.451635	45.509556
3502.704073	980456.378701	45.514561
3502.667132	980406.863830	45.519565
3502.353414	980359.152289	45.524570
3502.468743	980310.099882	45.529575
3502.560271	980263.102209	45.534580
3502.415415	980213.603437	45.539585
3502.600607	980156.137826	45.544589
3502.506245	980110.243990	45.549594
3502.945409	980053.810006	45.554599
3502.787548	980007.339713	45.559604
3502.695471	979952.750509	45.564609
3503.035857	979890.665559	45.569613
3502.760323	979851.148953	45.574618
3502.735411	979787.657776	45.579623
3502.989044	979729.492803	45.584628
3502.576119	979676.126045	45.589633
3502.692742	979617.591748	45.594637
3502.498450	979578.255250	45.599642
3502.829365	979517.437773	45.604647
3502.945325	979460.562718	45.609652
3502.560597	979409.924191	45.614657
3502.688048	979364.085520	45.619661
3502.471251	979326.802553	45.624666
3502.406624	979268.880702	45.629671
3502.458448	979222.857965	45.634676
3502.048422	979178.180979	45.639681
3502.449749	979127.410480	45.644685
3502.441958	979088.332982	45.649690
3502.543767	979025.105556	45.654695
3501.890649	978987.110643	45.659700
3502.190611	978940.165464	45.664705
3502.363166	978899.884568	45.669709
3502.098505	978864.169683	45.674714
3502.020917	978808.883251	45.679719
3502.453971	978774.127617	45.684724
3502.417532	978731.046558	45.689729
3502.575960	978678.162592	45.694733
3502.543307	978638.499884	45.699738
3502.584580	978575.765989	45.704743
3502.447242	978541.689131	45.709748
3502.463496	978493.321406	45.714753
3502.497689	978430.196248	45.719757
3502.175268	978400.252815	45.724762
3502.358525	978357.816726	45.729767
3502.315636	978299.002073	45.734772
3502.287710	978259.042820	45.739777
3502.375772	978210.758590	45.744781
3502.176516	978176.982894	45.749786
3501.894201	978131.397260	45.754791
3502.200354	978081.610305	45.759796
3502.423431	978047.177991	45.764801
3502.375300	977988.458724	45.769805
3502.041618	977951.381464	45.774810
3502.337378	977887.914088	45.779815
3502.627079	977775.098428	45.784820
3502.268594	977606.880762	45.789825
3502.422107	977388.146914	45.794829
3502.222367	977103.005608	45.799834
3502.052349	976751.579305	45.804839
3502.091104	976330.698469	45.809844
3501.724887	975865.864711	45.814849
3502.102086	975341.236285	45.819853
3501.544388	974741.136386	45.824858
3501.906379	974063.964615	45.829863
3501.434836	973329.737376	45.834868
3501.429083	972525.405626	45.839873
3501.446171	971659.328011	45.844877
3501.054094	970722.644283	45.849882
3501.021561	969709.419681	45.854887
3501.028807	968630.041387	45.859892
3500.837904	967458.862638	45.864897
3500.642940	966236.627075	45.869901
3500.111533	964921.243219	45.874906
3500.113483	963524.259711	45.879911
3499.777888	962061.635040	45.884916
3499.670989	960518.328043	45.889921
3499.470075	958882.072206	45.894925
3498.931099	957190.782652	45.899930
3498.658806	955395.261338	45.904935
3498.366176	953563.870995	45.909940
3497.859623	951659.387659	45.914945
3497.888669	949683.279309	45.919949
3497.456124	947641.854417	45.924954
3497.414794	945499.742853	45.929959
3496.971202	943273.053926	45.934964
3496.762160	940968.577024	45.939969
3496.027128	938587.202392	45.944973
3495.551568	936134.746618	45.949978
3495.150961	933587.720293	45.954983
3494.497742	930974.287866	45.959988
3494.242659	928278.105413	45.964993
3494.038101	925501.804897	45.969997
3493.533624	922653.313123	45.975002
3492.744904	919723.281340	45.980007
3492.354495	916687.011649	45.985012
3491.578317	913592.938875	45.990017
3491.374295	910414.592323	45.995021
3490.541136	907172.586549	46.000026
3490.137215	903838.267467	46.005031
3489.228684	900429.797594	46.010036
3488.492301	896939.696684	46.015041
3488.010762	893353.792959	46.020045
3487.427394	889720.563128	46.025050
3487.145552	885983.219471	46.030055
3486.128652	882178.088413	46.035060
3485.034649	878296.707186	46.040065
3485.066731	874321.865050	46.045069
3483.763226	870279.921452	46.050074
3483.306966	866146.988414	46.055079
3482.437886	861949.363963	46.060084
3481.584855	857662.156617	46.065089
3480.972875	853295.782468	46.070093
3479.866422	848846.327381	46.075098
3479.216137	844321.191064	46.080103
3478.463234	839717.652006	46.085108
3477.588090	835033.429153	46.090113
3476.718791	830267.920934	46.095117
3475.866881	825417.365554	46.100122
3474.918194	820485.155404	46.105127
3474.062466	815478.561080	46.110132
3473.229249	810389.629187	46.115137
3472.606050	805217.550126	46.120141
3471.472348	799963.674883	46.125146
3470.198685	794616.851279	46.130151
3469.199140	789201.524676	46.135156
3467.766160	783718.740213	46.140161
3467.076591	778126.160635	46.145165
3466.047558	772481.559807	46.150170
3465.035963	766733.933487	46.155175
3464.126736	760911.414096	46.160180
3462.981447	755003.428904	46.165185
3461.802028	749018.312596	46.170189
3460.663232	742954.854100	46.175194
3459.206379	736807.408369	46.180199
3457.986751	730575.465175	46.185204
3457.043346	724276.348113	46.190209
3455.920314	717877.560056	46.195213
3454.483845	711404.841405	46.200218
3453.403289	704844.480547	46.205223
3451.874297	698191.374055	46.210228
3450.350216	691484.387890	46.215233
3449.030747	684686.457261	46.220237
3447.896422	677801.262116	46.225242
3446.497433	670859.799248	46.230247
3445.312589	663819.789811	46.235252
3443.473295	656705.136118	46.240257
3442.360100	649513.352900	46.245261
3440.741190	642240.732405	46.250266
3439.569925	634891.609282	46.255271
3438.286325	627457.962519	46.260276
3436.623073	619944.887528	46.265281
3435.236086	612340.694371	46.270285
3433.619537	604686.659870	46.275290
3431.983538	596933.151367	46.280295
3430.215955	589093.385659	46.285300
3428.317138	581212.888537	46.290305
3426.780534	573216.804691	46.295309
3424.861981	565185.792124	46.300314
3423.347636	557051.273277	46.305319
3421.382265	548858.919157	46.310324
3419.675989	540578.591008	46.315329
3418.095762	532232.666913	46.320333
3416.119414	523814.355354	46.325338
3414.100626	515335.457618	46.330343
3412.086058	506764.125516	46.335348
3409.990576	498143.537160	46.340353
3407.994975	489451.687789	46.345357
3406.161855	480685.085520	46.350362
3404.310541	471847.624002	46.355367
3401.793411	462935.229911	46.360372
3399.860207	453982.000256	46.365377
3398.187300	444935.314351	46.370381
3395.530546	435837.006840	46.375386
3393.540372	426669.775594	46.380391
3391.329960	417439.086736	46.385396
3388.804258	408136.676337	46.390401
3386.883020	398766.381745	46.395405
3384.214901	389348.821215	46.400410
3381.742099	379864.554580	46.405415
3379.578350	370321.244845	46.410420
3376.749925	360727.309423	46.415425
3374.262242	351091.235930	46.420429
3371.749697	341387.447491	46.425434
3368.909793	331621.369977	46.430439
3366.050525	321829.856068	46.435444
3363.258325	311988.897511	46.440449
3360.545417	302070.187464	46.445453
3357.431514	292148.095878	46.450458
3354.376099	282160.264214	46.455463
3351.630720	272134.336190	46.460468
3348.436143	262078.420940	46.465473
3344.989321	251966.704677	46.470477
3341.902317	241853.916839	46.475482
3338.379399	231672.931779	46.480487
3334.865265	221437.722081	46.485492
3331.182848	211193.022022	46.490497
3327.716715	200935.585201	46.495501
3324.100083	190695.012923	46.500506
3320.302923	180429.677493	46.505511
3316.202446	170123.341135	46.510516
3311.932592	159837.529588	46.515521
3308.139884	149522.305626	46.520525
3303.414432	139230.198331	46.525530
3298.929351	128924.591455	46.530535
3294.316787	118641.296885	46.535540
3289.068220	108376.151337	46.540545
3284.207455	98112.227839	46.545549
3278.553663	87897.239917	46.550554
3272.762915	77708.420499	46.555559
3266.520732	67561.208171	46.560564
3259.118722	57490.236378	46.565569
3251.682881	47497.598348	46.570573
3241.639286	37655.872470	46.575578
3217.509910	28317.935860	46.580583
3169.305890	19914.133982	46.585588
3114.198181	12230.996963	46.590593
3060.868767	5382.388103	46.595597
2964.943960	714.774265	46.600602
2764.685970	404.728546	46.605607
2650.187090	406.240326	46.610612
2636.643529	392.414699	46.615617
2691.116319	364.618061	46.620621
2768.939500	349.903085	46.625626
2836.366774	347.811677	46.630631
2879.194848	357.683524	46.635636
2895.618052	362.117324	46.640641
2894.263315	356.481080	46.645645
2883.991993	335.237631	46.650650
2872.053165	333.523901	46.655655
2862.790747	339.778330	46.660660
2856.273365	349.172694	46.665665
2853.274500	341.447891	46.670669
2851.611054	341.247538	46.675674
2850.498623	342.528077	46.680679
2849.646035	327.594168	46.685684
2847.199690	335.270238	46.690689
2844.305476	331.454209	46.695693
2841.550708	340.235787	46.700698
2838.385151	339.036026	46.705703
2835.849908	325.540830	46.710708
2832.832298	328.671270	46.715713
2829.551498	323.649345	46.720717
2825.988723	324.667705	46.725722
2822.684814	323.818701	46.730727
2819.971411	323.335846	46.735732
2816.741599	321.778200	46.740737
2813.710367	323.753234	46.745741
2810.988535	317.069711	46.750746
2806.825381	313.695438	46.755751
2803.788973	315.953886	46.760756
2800.146581	318.000774	46.765761
2797.249177	309.372446	46.770765
2794.159849	309.066810	46.775770
2790.717099	305.073781	46.780775
2787.629416	303.408266	46.785780
2784.427474	308.345550	46.790785
2781.073600	313.488725	46.795789
2777.541566	303.709808	46.800794
2774.145121	304.532062	46.805799
2770.702162	303.510171	46.810804
2767.177931	307.523976	46.815809
2763.916732	306.647536	46.820813
2761.024598	300.279313	46.825818
2757.716451	300.559985	46.830823
2754.367679	294.457659	46.835828
2750.240099	297.807920	46.840833
2747.250548	285.295062	46.845837
2743.767676	300.023039	46.850842
2740.289128	296.930768	46.855847
2737.358677	287.960258	46.860852
2733.651006	289.365706	46.865857
2730.369564	296.971792	46.870861
2726.669467	289.215983	46.875866
2723.221516	294.774151	46.880871
2720.236513	282.988459	46.885876
2716.221032	296.309287	46.890881
2712.876007	285.464859	46.895885
2709.764666	287.294690	46.900890
2706.062184	292.843823	46.905895
2703.027806	285.672922	46.910900
2699.582030	285.982525	46.915905
2696.126472	281.082427	46.920909
2692.849129	279.554776	46.925914
2688.974024	284.725411	46.930919
2685.534477	284.093388	46.935924
2681.555038	286.098126	46.940929
2678.392050	281.104910	46.945933
2674.969708	285.363196	46.950938
2672.240242	276.517044	46.955943
2668.610960	269.942673	46.960948
2665.029085	281.215798	46.965953
2661.393128	271.819532	46.970957
2657.794841	279.281349	46.975962
2654.022762	278.705450	46.980967
2651.165339	275.319025	46.985972
2647.976507	278.279943	46.990977
2644.824855	271.879692	46.995981
2640.774774	280.307975	47.000986
2636.923385	278.885949	47.005991
2633.856323	273.252929	47.010996
2630.122264	281.818533	47.016001
2626.930427	276.722858	47.021005
2623.754084	275.325585	47.026010
2619.792996	274.996140	47.031015
2616.776878	269.650998	47.036020
2613.050092	276.949529	47.041025
2609.632824	262.637225	47.046029
2606.176074	274.821558	47.051034
2602.575835	264.428521	47.056039
2598.879981	264.697813	47.061044
2595.334647	271.083146	47.066049
2592.337940	264.975447	47.071053
2588.689675	262.214614	47.076058
2585.153015	260.286996	47.081063
2582.256066	267.419501	47.086068
2578.148612	260.736381	47.091073
2574.616135	268.579440	47.096077
2571.162141	262.707769	47.101082
2567.198780	259.203525	47.106087
2564.591651	260.255127	47.111092
2560.732799	260.550229	47.116097
2557.077541	265.165036	47.121101
2553.838255	255.728590	47.126106
2550.226798	263.346026	47.131111
2547.353395	254.986480	47.136116
2543.878799	256.105261	47.141121
2540.383552	264.935280	47.146125
2536.858225	261.383389	47.151130
2532.715616	257.072303	47.156135
2529.727411	259.279979	47.161140
2526.163863	255.320529	47.166145
2522.754069	258.805889	47.171149
2519.156764	254.872036	47.176154
2515.381669	265.858301	47.181159
2512.385516	261.549375	47.186164
2508.717882	251.300899	47.191169
2505.042917	248.782477	47.196173
2501.405785	258.198055	47.201178
2498.066738	262.409718	47.206183
2494.493181	254.250006	47.211188
2491.328136	253.023087	47.216193
2487.967893	255.330703	47.221197
2484.622578	247.917887	47.226202
2480.602540	253.100568	47.231207
2477.485565	246.182164	47.236212
2473.335242	257.223705	47.241217
2470.149333	244.618308	47.246221
2466.679884	243.238067	47.251226
2462.925010	248.343978	47.256231
2459.697728	240.256629	47.261236
2456.665681	257.140854	47.266241
2452.917946	250.512445	47.271245
2449.468433	253.685325	47.276250
2445.624121	260.209104	47.281255
2442.549058	246.088806	47.286260
2438.747823	250.280813	47.291265
2435.421437	250.188844	47.296269
2432.007228	242.895350	47.301274
2428.220297	249.639937	47.306279
2424.804961	246.439735	47.311284
2421.311813	255.971296	47.316289
2417.917922	243.318046	47.321293
2414.261810	255.657046	47.326298
2410.783020	247.699000	47.331303
2407.476912	247.768851	47.336308
2404.027284	252.368060	47.341313
2400.736270	245.789659	47.346317
2397.170466	244.221811	47.351322
2393.729288	242.866441	47.356327
2390.140344	241.966378	47.361332
2386.296453	239.791580	47.366337
2382.571718	237.452305	47.371341
2379.280688	242.805154	47.376346
2376.064331	245.199781	47.381351
2372.654812	241.013256	47.386356
2369.300774	246.666851	47.391361
2365.612428	236.118022	47.396365
2362.219363	238.637295	47.401370
2358.286873	242.767815	47.406375
2355.071549	236.927544	47.411380
2351.507565	246.707683	47.416385
2348.155466	238.571917	47.421389
2344.690299	240.653902	47.426394
2341.026420	235.718803	47.431399
2337.727049	235.206285	47.436404
2333.788768	243.619008	47.441409
2330.341400	238.490058	47.446413
2327.385398	232.293699	47.451418
2323.644055	244.813411	47.456423
2320.253803	226.557472	47.461428
2316.583065	236.543363	47.466433
2312.997664	239.299487	47.471437
2309.466950	227.165225	47.476442
2305.832612	240.946384	47.481447
2302.888506	242.898944	47.486452
2299.186601	236.320488	47.491457
2295.450762	233.654660	47.496461
2292.043782	227.912429	47.501466
2288.670606	238.901535	47.506471
2285.403393	232.593343	47.511476
2281.662249	231.901049	47.516481
2278.284554	238.440376	47.521485
2274.858004	234.320444	47.526490
2270.922180	238.814417	47.531495
2267.453251	234.740842	47.536500
2263.766504	235.968335	47.541505
2260.436134	229.742889	47.546509
2257.354093	233.372203	47.551514
2253.687577	231.529308	47.556519
2250.399075	226.662577	47.561524
2246.478269	230.305630	47.566529
2243.130695	220.741219	47.571533
2239.676059	222.910007	47.576538
2235.917050	233.018220	47.581543
2232.612046	231.526419	47.586548
2229.286338	230.329667	47.591553
2225.789647	226.178612	47.596557
2221.887293	222.394090	47.601562
2218.472047	234.517806	47.606567
2215.512865	223.827698	47.611572
2211.891479	236.190230	47.616577
2208.100136	232.350308	47.621581
2204.882246	228.384334	47.626586
2201.143599	230.790589	47.631591
2197.785382	218.993079	47.636596
2193.573341	229.578945	47.641601
2190.837089	223.650073	47.646605
2187.510143	219.220158	47.651610
2183.307151	223.647640	47.656615
2179.904823	221.468888	47.661620
2176.619353	227.161753	47.666625
2173.164601	221.812229	47.671629
2169.879567	220.549404	47.676634
2166.135452	227.848292	47.681639
2163.095988	218.997304	47.686644
2159.506808	228.113947	47.691649
2155.762104	224.723837	47.696653
2152.146580	219.512720	47.701658
2148.223403	228.321895	47.706663
2145.174205	221.472496	47.711668
2141.815679	221.053189	47.716673
2138.537251	226.392307	47.721677
2135.076361	215.390867	47.726682
2130.952979	216.352644	47.731687
2127.750754	214.042846	47.736692
2123.946922	237.373410	47.741697
2120.269856	225.537078	47.746701
2117.292430	220.617623	47.751706
2113.398986	219.137703	47.756711
2109.964150	219.522721	47.761716
2106.533900	227.941019	47.766721
2103.192264	213.094304	47.771725
2099.805142	212.777602	47.776730
2095.874893	219.808289	47.781735
2092.906275	210.871070	47.786740
2089.607515	227.729393	47.791745
2085.720905	222.108515	47.796749
2082.311927	214.783481	47.801754
2078.565064	219.073820	47.806759
2075.262352	217.270157	47.811764
2071.734843	226.691870	47.816769
2068.211752	217.265527	47.821773
2064.536076	218.780946	47.826778
2061.094868	218.457497	47.831783
2057.512874	219.448889	47.836788
2053.929659	225.872241	47.841793
2050.689893	217.387023	47.846797
2047.570702	208.900569	47.851802
2043.736194	213.894992	47.856807
2040.167507	207.967068	47.861812
2036.702067	219.406936	47.866817
2033.225897	210.812053	47.871821
2030.053960	213.066893	47.876826
2026.037919	216.184333	47.881831
2022.691329	213.182347	47.886836
2019.290551	213.900773	47.891841
2015.546377	216.763822	47.896845
2012.058458	203.204212	47.901850
2008.518074	216.683453	47.906855
2005.074962	207.998092	47.911860
2001.763793	214.315219	47.916865
1998.192050	217.473623	47.921869
1994.692963	212.476414	47.926874
1991.066820	218.471203	47.931879
1987.863170	206.240874	47.936884
1984.254144	216.130771	47.941889
1980.839155	215.396765	47.946893
1977.658858	208.228617	47.951898
1973.738233	209.553237	47.956903
1970.480436	202.539651	47.961908
1966.627061	211.326233	47.966913
1962.771535	217.471935	47.971917
1959.520128	209.919222	47.976922
1956.232721	214.724478	47.981927
1952.844533	208.072380	47.986932
1949.058031	210.497205	47.991937
1945.541196	214.681090	47.996941
1942.487858	205.803703	48.001946
1938.451344	207.530248	48.006951
1935.017274	206.799807	48.011956
1931.278623	200.313078	48.016961
1927.546966	214.176992	48.021965
1924.713674	207.208428	48.026970
1921.255182	215.378493	48.031975
1918.232509	206.833268	48.036980
1914.345526	216.868494	48.041985
1910.732487	207.245667	48.046989
1907.398241	203.782062	48.051994
1903.383661	208.202183	48.056999
1900.121389	201.380470	48.062004
1896.302785	206.120367	48.067009
1892.636336	213.657043	48.072013
1889.946102	200.082521	48.077018
1886.294380	206.564692	48.082023
1883.037725	196.719618	48.087028
1879.227352	203.863610	48.092033
1875.688970	208.973124	48.097037
1872.179030	211.446873	48.102042
1868.702309	213.860586	48.107047
1865.408210	197.596880	48.112052
1861.559769	204.924250	48.117057
1858.247130	205.937694	48.122061
1854.545997	202.398599	48.127066
1851.046509	207.357174	48.132071
1847.688831	205.749052	48.137076
1844.002891	204.108272	48.142081
1840.603038	201.245097	48.147085
1837.043582	206.791502	48.152090
1833.350936	201.438006	48.157095
1830.151500	202.619838	48.162100
1826.735111	202.177965	48.167105
1823.307950	207.692387	48.172109
1819.855778	199.547099	48.177114
1815.562206	198.439395	48.182119
1811.967550	204.401339	48.187124
1809.294817	201.189328	48.192129
1805.921137	199.214299	48.197133
1803.026213	198.026486	48.202138
1798.562264	210.468476	48.207143
1794.927665	194.380175	48.212148
1791.547694	194.695418	48.217153
1787.893879	199.866830	48.222157
1784.909018	192.793021	48.227162
1780.821787	204.456218	48.232167
1777.547820	198.233274	48.237172
1773.920347	200.553909	48.242177
1770.636606	203.340513	48.247181
1767.066538	205.370509	48.252186
1763.436918	205.635601	48.257191
1760.164033	199.623710	48.262196
1756.593865	194.988101	48.267201
1752.632589	201.862263	48.272205
1750.072487	192.721282	48.277210
1745.910543	198.488680	48.282215
1742.508061	200.123836	48.287220
1739.262898	194.113698	48.292225
1735.371562	198.840909	48.297229
1732.008529	190.570768	48.302234
1728.550717	193.716709	48.307239
1725.342867	191.991583	48.312244
1721.451231	198.678067	48.317249
1717.841298	194.142962	48.322253
1714.317888	184.676451	48.327258
1711.129963	192.269000	48.332263
1707.701306	194.513057	48.337268
1704.164518	197.534613	48.342273
1700.550836	194.034351	48.347277
1697.309126	188.034816	48.352282
1693.357447	202.401657	48.357287
1690.176844	188.394461	48.362292
1686.554727	195.767136	48.367297
1682.796469	193.330283	48.372301
1679.629999	198.582335	48.377306
1675.929828	194.140771	48.382311
1672.970400	187.299796	48.387316
1669.165110	194.452314	48.392321
1665.446698	205.290413	48.397325
1662.173116	197.267184	48.402330
1658.341531	201.307100	48.407335
1654.945453	199.706198	48.412340
1651.309012	197.053426	48.417345
1647.769271	199.279142	48.422349
1644.731688	189.354943	48.427354
1640.901469	207.410949	48.432359
1637.536844	195.337423	48.437364
1633.625579	201.245831	48.442369
1630.520317	199.394607	48.447373
1627.054549	193.248777	48.452378
1623.236535	193.836655	48.457383
1620.012650	192.243662	48.462388
1616.511014	194.371057	48.467393
1612.867043	195.533800	48.472397
1609.552648	191.641074	48.477402
1605.853270	192.353521	48.482407
1602.572117	188.204628	48.487412
1599.098583	188.132982	48.492417
1595.301232	192.523329	48.497421
1592.023952	189.408804	48.502426
1588.398901	186.200630	48.507431
1584.718491	188.066209	48.512436
1581.730357	187.070268	48.517441
1578.186847	194.043483	48.522445
1574.366859	189.410035	48.527450
1570.933248	191.972547	48.532455
1567.396110	191.080332	48.537460
1563.817478	186.094618	48.542465
1560.344748	187.918735	48.547469
1556.878667	186.261757	48.552474
1553.083227	191.184651	48.557479
1549.800481	190.586882	48.562484
1546.322056	185.939309	48.567489
1543.005097	188.028369	48.572493
1539.748065	186.065794	48.577498
1535.995849	197.166617	48.582503
1532.590663	187.091528	48.587508
1528.707179	186.145602	48.592513
1525.199249	189.376758	48.597517
1522.270669	191.091952	48.602522
1518.504550	198.524180	48.607527
1514.851429	196.662104	48.612532
1511.281594	201.443213	48.617537
1507.958179	196.946178	48.622541
1504.766036	184.375758	48.627546
1500.588902	197.079344	48.632551
1497.311751	184.139087	48.637556
1493.905494	194.564059	48.642561
1490.220740	189.335348	48.647565
1486.739732	182.973098	48.652570
1482.694779	196.818230	48.657575
1479.668945	184.434561	48.662580
1476.988839	197.800308	48.667585
1473.052657	190.586703	48.672589
1469.580496	185.869277	48.677594
1465.948853	192.255282	48.682599
1462.495562	190.311520	48.687604
1458.903392	190.367847	48.692609
1455.362067	191.505047	48.697613
1451.959233	192.249925	48.702618
1448.246536	191.437061	48.707623
1444.915565	194.091804	48.712628
1441.397375	192.024887	48.717633
1437.949574	194.077974	48.722637
1434.421470	187.932083	48.727642
1430.308405	193.499988	48.732647
1426.975551	193.059320	48.737652
1423.933077	188.723831	48.742657
1420.433124	194.177626	48.747661
1417.125361	189.966133	48.752666
1413.144899	180.129315	48.757671
1409.698232	188.491083	48.762676
1406.201573	180.505414	48.767681
1402.767905	192.380451	48.772685
1399.437597	177.568253	48.777690
1395.804631	192.639491	48.782695
1392.433670	191.833394	48.787700
1388.844900	183.021894	48.792705
1385.134989	187.321650	48.797709
1381.830565	178.828351	48.802714
1377.679609	188.824593	48.807719
1374.627442	179.725350	48.812724
1371.330154	180.372244	48.817729
1367.683066	188.003116	48.822733
1364.674388	178.046287	48.827738
1360.899900	186.837469	48.832743
1357.407131	178.579785	48.837748
1353.803596	183.045004	48.842753
1350.063993	178.478436	48.847757
1347.001521	182.117195	48.852762
1343.346591	179.373233	48.857767
1339.864347	171.715727	48.862772
1336.478035	174.161325	48.867777
1332.367309	189.465739	48.872781
1329.287840	170.456209	48.877786
1325.627326	179.658434	48.882791
1322.026853	181.895512	48.887796
1318.702390	174.908286	48.892801
1314.865911	182.586226	48.897805
1311.997960	179.466039	48.902810
1308.001840	179.471819	48.907815
1304.694467	169.012746	48.912820
1301.500314	183.298001	48.917825
1297.627290	177.234383	48.922829
1293.967238	177.527133	48.927834
1290.716681	181.400488	48.932839
1287.274265	189.917579	48.937844
1283.843219	184.287315	48.942849
1280.024930	181.471993	48.947853
1276.940537	185.861323	48.952858
1273.026246	180.875144	48.957863
1269.081985	178.749806	48.962868
1266.219621	178.779095	48.967873
1262.562584	186.181689	48.972877
1259.646721	173.618403	48.977882
1255.718269	184.701860	48.982887
1252.318498	177.528112	48.987892
1248.885209	175.180223	48.992897
1245.193483	184.386750	48.997901
1241.869662	175.722212	49.002906
1237.966115	175.905230	49.007911
1234.457456	179.722459	49.012916
1231.227521	181.834389	49.017921
1227.486574	180.668287	49.022925
1224.468326	176.692052	49.027930
1220.645177	189.593143	49.032935
1216.678290	170.199211	49.037940
1213.659193	177.846842	49.042945
1209.991994	178.196360	49.047949
1206.747619	175.244217	49.052954
1203.274072	175.083488	49.057959
1199.765585	171.616064	49.062964
1196.512317	175.898438	49.067969
1192.501243	181.122191	49.072973
1189.020701	178.051489	49.077978
1185.435361	176.997250	49.082983
1182.220187	180.457362	49.087988
1178.804749	176.597130	49.092993
1174.894316	173.034474	49.097997
1171.481228	176.611415	49.103002
1167.679994	180.712368	49.108007
1164.561973	175.395130	49.113012
1160.947860	172.482146	49.118017
1157.338795	181.991256	49.123021
1154.268069	176.751059	49.128026
1150.628895	177.360083	49.133031
1147.136691	177.502573	49.138036
1143.779716	179.181106	49.143041
1140.251061	177.541976	49.148045
1136.561362	169.841097	49.153050
1132.844777	178.611177	49.158055
1129.217514	178.812771	49.163060
1126.197492	175.286451	49.168065
1122.564453	178.812021	49.173069
1119.184394	175.613289	49.178074
1115.639140	184.814732	49.183079
1112.122775	180.682136	49.188084
1108.428888	181.415543	49.193089
1104.794244	175.770061	49.198093
1101.771107	177.107596	49.203098
1098.215912	176.471956	49.208103
1094.479525	174.216314	49.213108
1091.142727	175.139587	49.218113
1087.083270	166.344331	49.223117
1083.946365	172.305405	49.228122
1080.138696	170.312915	49.233127
1077.080664	173.994655	49.238132
1073.759597	174.420976	49.243137
1069.992755	177.822553	49.248141
1066.330653	164.455616	49.253146
1062.916755	172.479047	49.258151
1059.648295	169.043302	49.263156
1056.387042	167.808164	49.268161
1051.976676	174.977004	49.273165
1049.209498	171.564064	49.278170
1045.386796	175.135981	49.283175
1042.147682	169.948012	49.288180
1038.622470	170.801789	49.293185
1034.869370	171.233754	49.298189
1031.800507	177.463700	49.303194
1027.720670	172.166128	49.308199
1024.096744	170.709617	49.313204
1021.107196	161.668212	49.318209
1017.651416	171.577470	49.323213
1014.229545	163.340851	49.328218
1010.460537	168.070422	49.333223
1006.646068	165.334151	49.338228
1003.111097	169.897918	49.343233
999.649363	176.090731	49.348237
996.645721	156.223243	49.353242
992.949827	169.733417	49.358247
989.698981	167.690184	49.363252
986.395229	166.783418	49.368257
982.250792	165.671842	49.373261
978.928907	165.275460	49.378266
975.267785	170.153174	49.383271
971.871686	164.303635	49.388276
968.423501	169.941259	49.393281
964.538232	164.345139	49.398285
961.664616	165.177594	49.403290
957.913575	168.812307	49.408295
954.399865	171.569758	49.413300
950.803881	164.769837	49.418305
946.889145	177.719699	49.423309
943.991374	163.095659	49.428314
940.610385	161.141519	49.433319
937.172683	165.320680	49.438324
933.269407	164.094436	49.443329
929.803721	176.969666	49.448333
926.331110	166.121582	49.453338
922.536759	164.415652	49.458343
919.414535	163.456750	49.463348
916.229363	166.819186	49.468353
912.456358	171.674563	49.473357
909.029266	162.694811	49.478362
905.228936	173.824548	49.483367
901.673883	162.613626	49.488372
898.421006	166.746601	49.493377
894.397795	168.371296	49.498381
891.439337	164.799411	49.503386
887.595155	171.989986	49.508391
884.368284	165.233731	49.513396
881.326612	177.836229	49.518401
877.286947	167.939322	49.523405
874.107786	159.727726	49.528410
870.279573	160.888816	49.533415
866.765215	172.163332	49.538420
863.482995	165.085141	49.543425
859.585760	172.514554	49.548429
856.466739	158.824375	49.553434
852.655209	173.529378	49.558439
849.037184	163.655803	49.563444
845.831307	176.931619	49.568449
842.004313	169.140538	49.573453
838.554404	164.831782	49.578458
835.281386	163.483566	49.583463
831.876563	165.607685	49.588468
829.106180	164.869920	49.593473
824.982384	158.146188	49.598477
821.241646	167.665931	49.603482
817.518610	171.688839	49.608487
813.842883	169.533838	49.613492
810.840434	163.416452	49.618497
806.912877	173.891554	49.623501
803.833819	160.180600	49.628506
800.446431	164.757581	49.633511
796.641881	164.290644	49.638516
793.287003	153.871205	49.643521
789.823881	160.185287	49.648525
786.235251	161.216493	49.653530
782.498797	162.116927	49.658535
779.160521	161.321924	49.663540
776.073106	163.741906	49.668545
771.899307	159.661252	49.673549
768.691334	159.121266	49.678554
765.448943	168.580541	49.683559
761.428959	170.311132	49.688564
758.083296	165.256538	49.693569
754.567162	174.172844	49.698573
751.121543	157.128522	49.703578
747.673029	170.426086	49.708583
743.984831	170.107284	49.713588
740.644228	160.458282	49.718593
737.358154	161.417548	49.723597
733.656660	157.808135	49.728602
730.073583	161.152212	49.733607
726.576461	154.634440	49.738612
723.408540	151.662723	49.743617
719.912452	164.490954	49.748621
716.223899	164.308568	49.753626
712.694798	162.992545	49.758631
708.995129	158.689497	49.763636
705.836944	161.675935	49.768641
702.173864	169.260120	49.773645
698.775146	162.342242	49.778650
694.880686	160.810038	49.783655
691.498817	167.907783	49.788660
688.068826	157.479996	49.793665
684.342988	157.979080	49.798669
681.082868	156.687316	49.803674
677.409650	156.819102	49.808679
674.287781	157.969702	49.813684
671.258080	161.449817	49.818689
667.039882	160.200667	49.823693
663.339977	151.938266	49.828698
659.873469	158.834932	49.833703
656.722731	155.569673	49.838708
653.234005	153.956970	49.843713
649.715892	162.630162	49.848717
646.242097	155.778879	49.853722
642.428527	147.882138	49.858727
638.908843	153.807752	49.863732
635.598948	147.531502	49.868737
631.869029	162.003896	49.873741
628.538969	156.312548	49.878746
624.806109	162.150161	49.883751
621.607799	156.019548	49.888756
618.296993	152.262217	49.893761
614.919482	164.302284	49.898765
611.579701	163.882701	49.903770
607.462537	157.745418	49.908775
603.791705	158.369040	49.913780
600.464371	158.825240	49.918785
596.844445	150.088363	49.923789
593.819257	151.488117	49.928794
590.302457	160.303180	49.933799
586.666147	158.259991	49.938804
583.248116	148.553343	49.943809
579.063702	155.162753	49.948813
575.589781	154.163846	49.953818
572.516872	155.273357	49.958823
568.874670	151.009937	49.963828
565.951811	146.323749	49.968833
562.271281	147.886120	49.973837
558.665119	154.786560	49.978842
554.976137	162.650732	49.983847
551.560463	159.939038	49.988852
548.162760	152.556915	49.993857
544.121961	157.772603	49.998861
540.933794	159.529598	50.003866
537.407647	154.126405	50.008871
533.700897	160.241608	50.013876
530.723569	152.053502	50.018881
526.701209	168.916021	50.023885
523.573723	155.072364	50.028890
519.826944	151.239019	50.033895
515.931508	160.596120	50.038900
513.153538	154.705322	50.043905
509.795937	161.948697	50.048909
506.434913	155.874326	50.053914
502.647997	163.222457	50.058919
498.977291	154.491858	50.063924
495.176109	154.516533	50.068929
491.840839	151.540516	50.073933
488.516582	153.139476	50.078938
484.870920	166.081692	50.083943
481.418659	158.521470	50.088948
477.998145	153.788784	50.093953
474.408118	159.086420	50.098957
470.963592	150.543315	50.103962
467.555515	154.856117	50.108967
463.883458	152.664312	50.113972
460.565931	154.977028	50.118977
457.023742	148.297377	50.123981
453.448496	151.734910	50.128986
449.924749	152.601183	50.133991
446.121487	153.876779	50.138996
443.437228	145.073738	50.144001
439.402045	149.151462	50.149005
435.978901	143.087695	50.154010
432.197735	152.705249	50.159015
428.300926	150.127068	50.164020
425.464048	148.743027	50.169025
421.779230	153.772813	50.174029
418.425420	154.739577	50.179034
414.947010	155.147231	50.184039
411.022836	152.627447	50.189044
407.949465	152.594392	50.194049
404.712712	156.106258	50.199053
401.280627	139.948454	50.204058
397.368926	149.931201	50.209063
393.700913	147.069892	50.214068
390.550270	144.553055	50.219073
386.777602	139.908888	50.224077
383.079156	149.208350	50.229082
379.731755	149.131788	50.234087
376.416864	141.559601	50.239092
373.093999	147.607319	50.244097
369.359494	140.999747	50.249101
365.714891	143.627581	50.254106
362.321139	148.597671	50.259111
358.579267	139.565109	50.264116
355.518310	136.235261	50.269121
351.754903	154.288146	50.274125
348.327623	146.866342	50.279130
344.953823	149.999154	50.284135
340.846708	152.315107	50.289140
337.742461	157.377077	50.294145
333.968331	148.046395	50.299149
330.497575	144.077201	50.304154
327.610820	151.652183	50.309159
323.984952	153.179412	50.314164
320.409358	153.137522	50.319169
316.909250	147.759759	50.324173
313.383937	156.493481	50.329178
309.652252	142.605557	50.334183
305.927721	146.353730	50.339188
302.804831	153.706694	50.344193
298.878752	149.283657	50.349197
296.030925	152.013507	50.354202
292.497300	144.515389	50.359207
288.535714	146.841070	50.364212
285.398536	151.975587	50.369217
281.519740	158.991547	50.374221
278.257039	157.201422	50.379226
274.817499	146.230616	50.384231
271.042638	152.910555	50.389236
267.729843	152.215196	50.394241
264.090795	139.911294	50.399245
260.635550	145.799804	50.404250
257.142114	154.894292	50.409255
253.535152	153.081346	50.414260
250.290363	146.733298	50.419265
246.828562	154.168126	50.424269
243.192227	151.553440	50.429274
239.858987	143.581854	50.434279
236.155606	150.553758	50.439284
232.867733	138.734358	50.444289
228.894503	149.415076	50.449293
225.665334	154.207689	50.454298
222.044073	144.961434	50.459303
218.434299	151.087506	50.464308
215.172585	142.733177	50.469313
211.418984	153.280838	50.474317
208.088889	142.759716	50.479322
205.078173	154.765871	50.484327
201.580142	156.843946	50.489332
197.906598	139.384481	50.494337
194.296100	150.416968	50.499341
190.755168	144.518226	50.504346
187.306252	149.132393	50.509351
183.678734	158.279259	50.514356
179.970159	141.982317	50.519361
176.071125	157.975287	50.524365
173.267426	155.982803	50.529370
169.783781	145.728680	50.534375
166.223264	157.949703	50.539380
162.633356	148.715175	50.544385
159.377779	155.559164	50.549389
155.524244	150.691438	50.554394
152.233632	149.690197	50.559399
148.532020	154.604121	50.564404
145.079113	147.828621	50.569409
141.559570	160.671513	50.574413
137.923778	148.135711	50.579418
134.545916	148.631673	50.584423
131.135286	151.673305	50.589428
127.379073	143.841033	50.594433
124.187014	143.782839	50.599437
120.567872	144.500694	50.604442
117.286689	141.752522	50.609447
113.496419	148.064838	50.614452
110.334899	140.205541	50.619457
106.415055	151.247848	50.624461
103.094966	141.466036	50.629466
99.565494	147.621812	50.634471
95.939784	158.121268	50.639476
92.427779	149.553642	50.644481
88.976293	151.302768	50.649485
85.650144	146.257673	50.654490
82.254217	149.936674	50.659495
78.595412	148.271600	50.664500
75.160853	154.389312	50.669505
71.078717	149.743210	50.674509
67.463862	145.830144	50.679514
64.502534	148.804863	50.684519
60.836592	158.209902	50.689524
57.793563	146.157181	50.694529
54.015714	141.726783	50.699533
50.768730	151.155424	50.704538
47.367834	145.821610	50.709543
43.712473	159.742983	50.714548
40.201657	145.407960	50.719553
36.281579	151.246328	50.724557
33.002847	140.044207	50.729562
29.675618	139.890407	50.734567
25.762689	155.731048	50.739572
22.622995	150.851498	50.744577
19.224341	145.532129	50.749581
15.756081	139.601857	50.754586
12.073535	143.771806	50.759591
7.638514	155.787388	50.764596
5.279925	146.817894	50.769601
1.429262	158.222726	50.774605