Thu Jun 16 10:48:59 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.380069	94.151187	0.000000
0.652431	89.506873	0.005005
0.562185	83.371248	0.010010
0.433091	84.941800	0.015014
-0.061411	66.562738	0.020019
-0.148609	65.082790	0.025024
-0.227445	52.212357	0.030029
-0.586201	46.216619	0.035034
-0.725603	30.473548	0.040038
-0.954565	16.461769	0.045043
-1.430372	15.485550	0.050048
-1.734939	-7.705863	0.055053
-2.003142	-5.422644	0.060058
-2.165573	-10.889960	0.065062
-2.243871	-13.384147	0.070067
-2.717467	-13.868745	0.075072
-3.057018	-16.982017	0.080077
-3.773160	-12.213090	0.085082
-4.513534	-11.011117	0.090086
-4.370840	-11.992572	0.095091
-4.696285	-14.733392	0.100096
-4.733576	-17.649982	0.105101
-4.335484	-15.219788	0.110106
-4.702101	-11.528897	0.115110
-5.406604	-14.474720	0.120115
-5.767104	-5.661566	0.125120
-6.364984	-5.494438	0.130125
-5.994176	-12.246249	0.135130
-6.160160	-7.528877	0.140134
-6.632670	-2.607539	0.145139
-7.395278	-5.424785	0.150144
-7.423186	-10.728567	0.155149
-7.909866	-12.467156	0.160154
-7.670528	-12.495016	0.165158
-7.554338	-12.328500	0.170163
-8.189491	-10.030414	0.175168
-7.804634	-12.495585	0.180173
-8.652132	-11.691634	0.185178
-9.416044	-2.927925	0.190182
-9.280045	-16.790545	0.195187
-9.254672	-13.942812	0.200192
-9.383072	-4.461459	0.205197
-9.602870	-13.158186	0.210202
-10.408053	-12.831015	0.215206
-10.630347	-21.899347	0.220211
-11.001211	-15.270054	0.225216
-11.005813	-15.920946	0.230221
-10.982431	-23.484076	0.235226
-11.217208	-2.127591	0.240230
-11.275067	-15.122086	0.245235
-11.999312	-6.016391	0.250240
-12.114259	-13.400300	0.255245
-12.018567	-15.749316	0.260250
-12.868927	-9.937339	0.265254
-13.111022	-13.935164	0.270259
-13.894402	-15.606369	0.275264
-14.012857	-15.753959	0.280269
-14.128253	-10.944224	0.285274
-13.620865	-16.214237	0.290278
-13.727711	-19.563864	0.295283
-13.738700	-9.579056	0.300288
-14.333312	-11.123316	0.305293
-14.987523	-9.642679	0.310298
-15.187330	-17.285931	0.315302
-15.183067	-21.458045	0.320307
-15.646592	-18.922649	0.325312
-16.647039	-16.500266	0.330317
-16.470293	-22.735612	0.335322
-16.564324	-14.168444	0.340326
-16.887527	-11.318251	0.345331
-17.329373	-17.005849	0.350336
-17.401321	-13.444750	0.355341
-17.119146	-17.015528	0.360346
-17.699120	-4.595934	0.365350
-17.405160	-7.801572	0.370355
-18.213640	-6.898706	0.375360
-18.661831	-3.286869	0.380365
-18.333219	-20.954320	0.385370
-18.444272	-10.572469	0.390374
-19.294532	-15.411334	0.395379
-20.129811	-7.777648	0.400384
-20.452847	-19.236969	0.405389
-19.585213	-25.605532	0.410394
-20.098161	-6.032708	0.415398
-20.074159	-21.250958	0.420403
-20.697538	-16.261185	0.425408
-20.690446	-21.522998	0.430413
-21.559954	-10.927803	0.435418
-21.875710	-11.673871	0.440422
-22.215224	-10.309071	0.445427
-22.563365	-5.142417	0.450432
-22.484499	-11.098284	0.455437
-22.485791	-3.018100	0.460442
-22.424013	-10.576039	0.465446
-21.971186	-10.579695	0.470451
-22.563419	-5.135044	0.475456
-23.111168	-14.340684	0.480461
-23.458303	-19.965995	0.485466
-24.046976	-19.909005	0.490470
-24.770049	-10.259532	0.495475
-24.954976	-11.657716	0.500480
-24.843546	-16.124560	0.505485
-25.205564	-16.778536	0.510490
-25.287973	-15.903916	0.515494
-25.293766	-22.102879	0.520499
-25.702278	-20.080694	0.525504
-25.550533	-22.335681	0.530509
-25.983750	-17.725878	0.535514
-26.293092	-18.267017	0.540518
-26.471918	-21.555125	0.545523
-27.222016	-16.656874	0.550528
-27.503288	-16.888343	0.555533
-27.802323	-18.016398	0.560538
-28.186189	-6.015837	0.565542
-28.298278	-11.957509	0.570547
-28.475291	-8.397790	0.575552
-29.037400	-16.275447	0.580557
-28.509345	-23.834969	0.585562
-28.689004	-12.750617	0.590566
-28.733657	-15.054537	0.595571
-29.325707	-19.122477	0.600576
-29.750925	-14.150851	0.605581
-29.773204	-16.148598	0.610586
-30.458518	-3.895188	0.615590
-30.404876	-13.194594	0.620595
-30.266701	-13.756716	0.625600
-30.875553	-7.062832	0.630605
-31.676329	-13.899023	0.635610
-31.944674	-5.893880	0.640614
-31.960320	-17.942156	0.645619
-32.109269	-9.268343	0.650624
-32.002716	-6.032802	0.655629
-31.751403	-13.068025	0.660634
-32.843210	2.933034	0.665638
-33.369554	-18.193779	0.670643
-33.622913	0.035208	0.675648
-33.854538	-11.470694	0.680653
-33.680895	-11.431564	0.685658
-33.730030	-5.344463	0.690662
-33.679859	-2.674063	0.695667
-34.332343	-3.057274	0.700672
-34.893036	-11.451717	0.705677
-34.757613	-15.200087	0.710682
-35.356201	-4.215389	0.715686
-35.112432	-15.810114	0.720691
-36.256849	-15.962564	0.725696
-36.855089	-16.365493	0.730701
-36.379339	-6.726899	0.735706
-36.197104	-12.997191	0.740710
-36.442863	-15.228412	0.745715
-36.621116	-18.088163	0.750720
-37.069713	-7.394423	0.755725
-37.577776	-12.726184	0.760730
-38.179440	-4.098991	0.765734
-37.856707	-10.995177	0.770739
-38.457743	-6.193969	0.775744
-38.478628	-1.671741	0.780749
-38.255202	-17.612143	0.785754
-38.937664	-15.381213	0.790758
-39.370158	-13.733794	0.795763
-40.177130	-6.325374	0.800768
-39.943418	-17.716985	0.805773
-39.933929	-13.184291	0.810778
-40.056001	6.881242	0.815782
-40.038389	-10.485818	0.820787
-40.952926	-3.756606	0.825792
-41.236232	-13.977486	0.830797
-41.260266	-12.354362	0.835802
-41.824563	-1.188874	0.840806
-41.795935	-11.591334	0.845811
-41.775613	-12.284918	0.850816
-41.962877	-10.114519	0.855821
-42.476514	-10.174500	0.860826
-43.126135	1.778139	0.865830
-43.136115	-12.139968	0.870835
-43.401265	-14.701631	0.875840
-43.373067	-20.297125	0.880845
-43.185518	-15.132388	0.885850
-43.946267	-9.007493	0.890854
-44.176291	-15.243389	0.895859
-44.667522	-12.482922	0.900864
-44.868463	-13.557539	0.905869
-44.592349	-12.489816	0.910874
-45.435844	-8.200404	0.915878
-46.240816	-11.449846	0.920883
-46.504906	-9.857388	0.925888
-46.193833	-19.887046	0.930893
-46.054408	-15.010120	0.935898
-46.490498	-18.753218	0.940902
-46.344445	-29.032913	0.945907
-46.416570	-10.162458	0.950912
-47.552057	-20.850988	0.955917
-47.878504	-22.585372	0.960922
-48.478960	-17.970521	0.965926
-48.426343	-20.291107	0.970931
-48.362625	-19.294827	0.975936
-48.512048	-6.365225	0.980941
-48.158856	-14.051528	0.985946
-48.362903	-13.291269	0.990950
-49.235483	-10.612994	0.995955
-49.792813	-6.767167	1.000960
-50.080675	-11.340369	1.005965
-50.224624	-14.693335	1.010970
-50.211230	-3.292835	1.015974
-49.945885	-19.483441	1.020979
-51.231532	-7.185077	1.025984
-51.462567	-6.441568	1.030989
-51.524185	-17.870888	1.035994
-51.904294	-13.719424	1.040998
-51.576122	-28.896480	1.046003
-51.592439	-11.156445	1.051008
-51.646025	-9.504267	1.056013
-52.071991	-6.191668	1.061018
-52.492035	-15.045399	1.066022
-52.802278	-13.189011	1.071027
-53.512678	-13.925100	1.076032
-54.155970	-11.817448	1.081037
-54.332473	-7.392524	1.086042
-54.376943	-3.569502	1.091046
-54.440984	-8.768459	1.096051
-54.309021	-14.330790	1.101056
-54.370179	-0.565379	1.106061
-54.401182	-14.271554	1.111066
-55.524615	-15.654125	1.116070
-55.502852	-8.945291	1.121075
-55.835216	-14.795407	1.126080
-56.328134	-14.540161	1.131085
-56.118170	-10.757317	1.136090
-56.399392	-6.835877	1.141094
-56.694769	-11.192969	1.146099
-57.327546	-9.017109	1.151104
-57.577098	-6.412895	1.156109
-57.739466	-13.171490	1.161114
-57.986230	-6.161382	1.166118
-57.928837	-9.650026	1.171123
-57.934174	-12.060872	1.176128
-58.632108	-10.877154	1.181133
-58.849537	-17.308589	1.186138
-59.069624	-14.918983	1.191142
-59.424279	-16.068920	1.196147
-59.503299	-12.631252	1.201152
-59.650172	-7.386976	1.206157
-59.796893	-16.754283	1.211162
-60.768679	-9.739282	1.216166
-60.824299	-13.310763	1.221171
-61.261108	-14.627953	1.226176
-61.283420	-9.857773	1.231181
-60.765813	-22.513781	1.236186
-60.957343	-13.847141	1.241190
-61.385520	-10.664499	1.246195
-62.393567	-10.698408	1.251200
-62.725175	-10.960918	1.256205
-62.497738	-15.126015	1.261210
-62.644904	-2.722114	1.266214
-62.669100	-13.953408	1.271219
-63.253215	-9.727383	1.276224
-63.969977	-12.262746	1.281229
-63.808404	-13.480243	1.286234
-63.833993	-10.454799	1.291238
-64.247103	-11.232425	1.296243
-64.558145	-8.772343	1.301248
-64.804101	-14.796064	1.306253
-65.321798	-13.711980	1.311258
-65.726469	-5.218663	1.316262
-65.852583	-12.561260	1.321267
-65.832227	-5.002392	1.326272
-66.054074	-15.592029	1.331277
-65.834420	-3.817787	1.336282
-66.299524	-5.710976	1.341286
-66.964721	-4.537402	1.346291
-67.052853	-7.105137	1.351296
-67.493255	-11.263249	1.356301
-67.091102	-14.890556	1.361306
-67.777076	-15.790992	1.366310
-68.472355	-8.021413	1.371315
-68.945345	-8.501468	1.376320
-69.119979	-9.121496	1.381325
-69.072366	-10.261854	1.386330
-69.277292	-11.966897	1.391334
-68.997251	-6.360484	1.396339
-68.968148	-15.251054	1.401344
-69.381465	-10.901529	1.406349
-69.807857	-10.711536	1.411354
-70.733027	-6.163864	1.416358
-70.832935	-18.692363	1.421363
-70.920195	-6.596991	1.426368
-70.781262	-9.954781	1.431373
-71.217869	-14.415200	1.436378
-72.123250	-18.427798	1.441382
-72.150300	-16.063486	1.446387
-72.386595	-14.017574	1.451392
-72.419121	-11.027585	1.456397
-72.238919	-19.388100	1.461402
-72.421187	-6.519171	1.466406
-72.724206	-16.830210	1.471411
-73.349917	-13.765072	1.476416
-73.958608	-9.638670	1.481421
-73.914246	-14.804043	1.486426
-74.108563	-8.603472	1.491430
-74.159957	-15.694814	1.496435
-74.257323	-10.338463	1.501440
-75.079454	-14.545553	1.506445
-75.115394	-13.412249	1.511450
-75.696462	-10.222390	1.516454
-75.651231	-23.734277	1.521459
-75.626346	-12.813069	1.526464
-75.689591	-17.606688	1.531469
-76.709985	-14.783229	1.536474
-76.783860	-11.779106	1.541478
-76.855838	-16.764248	1.546483
-77.124982	-11.595262	1.551488
-77.345895	-12.710871	1.556493
-76.941976	-15.213723	1.561498
-77.878943	-17.661883	1.566502
-78.450984	-21.102629	1.571507
-78.724472	-15.740355	1.576512
-78.655400	-12.328249	1.581517
-78.590479	-17.325460	1.586522
-79.010748	-12.954661	1.591526
-79.103079	-18.737208	1.596531
-79.358652	-12.394615	1.601536
-79.983968	-15.323524	1.606541
-80.019313	-14.770696	1.611546
-80.306213	-6.979625	1.616550
-80.647499	-11.378848	1.621555
-81.078168	-7.221689	1.626560
-82.031705	-4.980086	1.631565
-81.394460	-16.202409	1.636570
-81.754365	-4.212915	1.641574
-82.074515	-5.160000	1.646579
-82.086127	-5.093707	1.651584
-82.235296	-4.328705	1.656589
-81.872389	-7.027316	1.661594
-82.331578	-6.949793	1.666598
-83.196494	-8.267553	1.671603
-83.312853	-6.082531	1.676608
-83.820531	-7.629116	1.681613
-83.626450	0.671721	1.686618
-84.583840	-3.689605	1.691622
-84.949037	-0.608919	1.696627
-84.755700	-4.603730	1.701632
-84.961631	-13.384523	1.706637
-84.819902	-5.017323	1.711642
-85.189977	2.898978	1.716646
-84.998542	-14.831726	1.721651
-85.647838	-12.713312	1.726656
-86.382065	-5.578639	1.731661
-86.342406	-19.601322	1.736666
-86.670713	-2.423442	1.741670
-87.119516	-9.114571	1.746675
-86.984526	-5.878011	1.751680
-87.446705	-13.391373	1.756685
-88.027235	-20.218767	1.761690
-88.458379	-8.921789	1.766694
-88.624332	-16.911376	1.771699
-88.498277	-12.282821	1.776704
-88.533451	-6.552987	1.781709
-88.603503	-11.571595	1.786714
-88.738979	-2.785078	1.791718
-88.929111	-17.281006	1.796723
-89.323661	-15.089863	1.801728
-89.942652	-5.176426	1.806733
-90.075198	-7.219086	1.811738
-90.172958	-8.281158	1.816742
-90.539979	-7.212800	1.821747
-91.356232	-6.143889	1.826752
-91.545011	-13.736670	1.831757
-91.431842	-15.150774	1.836762
-91.633248	-12.879581	1.841766
-91.617911	-11.142508	1.846771
-91.729706	-19.379589	1.851776
-92.431784	-7.230550	1.856781
-92.655244	-18.836144	1.861786
-93.070633	-11.579553	1.866790
-92.921687	-5.848580	1.871795
-93.200680	-1.697053	1.876800
-94.031306	-4.395116	1.881805
-94.341180	-7.774522	1.886810
-94.570202	-13.824913	1.891814
-94.703651	-12.257301	1.896819
-94.821653	-27.063665	1.901824
-95.162998	-14.073449	1.906829
-94.623102	-15.279484	1.911834
-95.125207	-14.992529	1.916838
-95.172633	-11.468731	1.921843
-95.620450	-20.257683	1.926848
-96.260754	-14.444510	1.931853
-96.317399	-24.752656	1.936858
-96.679511	-16.081997	1.941862
-96.766912	-24.526726	1.946867
-97.525251	-29.355410	1.951872
-98.051100	-17.685661	1.956877
-98.055816	-24.230280	1.961882
-98.202854	-15.169872	1.966886
-98.339789	-11.831054	1.971891
-98.212955	-20.855760	1.976896
-98.715632	-21.602893	1.981901
-98.628695	-20.346456	1.986906
-98.596533	-9.590907	1.991910
-99.190394	-22.683741	1.996915
-99.918957	-16.895475	2.006912
-99.454740	-19.476507	2.016909
-98.944199	-25.374114	2.026906
-98.474429	-23.565259	2.036902
-97.822015	-20.769901	2.046899
-97.610576	-14.050882	2.056896
-96.952845	-18.026365	2.066893
-95.875914	-17.876503	2.076890
-95.375442	-14.261299	2.086886
-95.526562	-16.851707	2.096883
-95.569602	-18.102499	2.106880
-94.481877	-12.857587	2.116877
-93.643951	-16.271014	2.126874
-92.819233	-13.424861	2.136870
-92.731160	-13.355203	2.146867
-92.624590	-15.075181	2.156864
-92.252500	-6.664833	2.166861
-91.374444	-12.312524	2.176858
-90.940189	-12.336433	2.186854
-89.844586	-8.423284	2.196851
-89.689331	-9.672129	2.206848
-89.600609	-10.263958	2.216845
-89.260328	-15.402557	2.226842
-88.224668	-3.524078	2.236838
-87.910528	-10.325959	2.246835
-87.149475	-10.167944	2.256832
-86.580886	-6.048365	2.266829
-86.508226	-16.539317	2.276826
-86.060454	-12.387276	2.286822
-85.473233	-9.295221	2.296819
-85.069727	-1.104166	2.306816
-83.999741	-4.398197	2.316813
-83.372350	-10.961684	2.326810
-83.206275	-3.638335	2.336806
-83.383578	-6.892317	2.346803
-82.179975	-1.750315	2.356800
-81.581397	-6.246323	2.366797
-81.534942	-11.588102	2.376794
-81.009586	-11.693200	2.386790
-80.444690	-3.867634	2.396787
-79.892252	-11.081941	2.406784
-78.708814	-14.709432	2.416781
-78.403034	-11.059726	2.426778
-78.825000	-8.087833	2.436774
-78.149571	-7.410605	2.446771
-77.396814	-2.296474	2.456768
-77.019921	-9.113221	2.466765
-76.195162	-14.526341	2.476762
-75.973161	-8.409890	2.486758
-75.248842	-12.992564	2.496755
-74.731130	-11.726471	2.506752
-74.312218	-10.519023	2.516749
-73.761559	-11.168973	2.526746
-72.938203	-18.593311	2.536742
-72.582444	-13.533834	2.546739
-72.502542	-14.509100	2.556736
-72.394729	-13.934187	2.566733
-71.118233	-14.797691	2.576730
-70.997739	-11.034832	2.586726
-70.217736	-7.793129	2.596723
-69.390071	-11.640329	2.606720
-69.442644	-18.459043	2.616717
-69.071859	-14.553968	2.626714
-68.252713	-15.886458	2.636710
-67.923731	-17.601954	2.646707
-67.060284	-12.446110	2.656704
-66.112696	-18.604768	2.666701
-66.199213	-16.074447	2.676698
-66.208811	-14.565527	2.686694
-65.608222	-12.103722	2.696691
-64.928250	-11.511058	2.706688
-64.053600	-7.625049	2.716685
-63.342858	-7.239919	2.726682
-62.992591	-9.509482	2.736678
-63.013602	-12.790629	2.746675
-63.029038	-14.595496	2.756672
-61.988011	-21.165603	2.766669
-60.869021	-21.364267	2.776666
-60.272012	-12.169390	2.786662
-60.258940	-11.086006	2.796659
-59.831897	-14.144568	2.806656
-59.659514	-14.103365	2.816653
-58.743899	-9.519234	2.826650
-58.038724	-17.949422	2.836646
-58.006023	-17.804776	2.846643
-57.009037	-8.485109	2.856640
-56.553451	-14.774485	2.866637
-56.600564	-8.909105	2.876634
-55.719318	-8.231761	2.886630
-55.268877	-12.481819	2.896627
-55.117775	-10.273427	2.906624
-54.151815	-12.164133	2.916621
-53.548717	-13.759970	2.926618
-53.453261	-9.806772	2.936614
-52.401726	-11.407132	2.946611
-52.117421	-5.552221	2.956608
-52.144684	-7.682638	2.966605
-51.096590	-7.578923	2.976602
-50.304435	-13.010557	2.986598
-50.368692	-14.776882	2.996595
-50.238923	-6.482699	3.006592
-49.084872	-10.719147	3.016589
-48.926784	-13.645987	3.026586
-48.017866	-17.710938	3.036582
-47.683242	-8.394410	3.046579
-47.660140	-10.665515	3.056576
-46.416347	-10.986249	3.066573
-45.596747	-14.442032	3.076570
-45.865882	-9.199214	3.086566
-45.714920	-3.886001	3.096563
-44.970874	-4.237936	3.106560
-44.286733	-11.438645	3.116557
-43.971026	-11.214580	3.126554
-42.973415	-17.438895	3.136550
-42.766250	-15.343042	3.146547
-42.162028	-13.459597	3.156544
-41.132046	-5.664512	3.166541
-41.074995	-9.443570	3.176538
-40.774821	-13.200380	3.186534
-40.617845	-18.592725	3.196531
-39.649776	-22.595242	3.206528
-38.993038	-29.852114	3.216525
-38.934897	-25.359243	3.226522
-37.926220	-18.540241	3.236518
-37.641659	-14.636125	3.246515
-37.576005	-17.366032	3.256512
-36.622651	-26.253094	3.266509
-36.141845	-20.102960	3.276506
-35.898733	-22.207630	3.286502
-34.896721	-20.627788	3.296499
-34.701037	-18.084542	3.306496
-34.317263	-24.624059	3.316493
-33.845040	-25.304604	3.326490
-32.906177	-24.367408	3.336486
-32.922587	-20.862457	3.346483
-32.407296	-24.376059	3.356480
-31.177756	-26.620193	3.366477
-30.977132	-20.993220	3.376474
-30.951174	-16.866241	3.386470
-30.375510	-17.102679	3.396467
-29.443003	-19.628933	3.406464
-29.616088	-16.238652	3.416461
-28.460362	-20.082327	3.426458
-27.968325	-20.992204	3.436454
-28.111109	-19.821473	3.446451
-27.265507	-14.209274	3.456448
-26.414264	-22.578797	3.466445
-26.224756	-16.105812	3.476442
-25.638412	-17.134450	3.486438
-24.794519	-10.674931	3.496435
-24.502443	-12.682691	3.506432
-24.411196	-19.773014	3.516429
-24.192519	-11.718249	3.526426
-23.194269	-19.378381	3.536422
-22.328136	-17.948254	3.546419
-21.757489	-15.980679	3.556416
-21.598983	-11.820139	3.566413
-21.524500	-17.354628	3.576410
-20.800301	-22.689680	3.586406
-20.210784	-11.052957	3.596403
-20.005472	-19.230732	3.606400
-19.006603	-23.790416	3.616397
-18.132034	-21.025984	3.626394
-18.197532	-24.293604	3.636390
-18.013939	-19.087332	3.646387
-16.841486	-20.947704	3.656384
-16.669087	-20.705337	3.666381
-16.262190	-23.007618	3.676378
-15.309239	-22.303299	3.686374
-15.234734	-21.464077	3.696371
-15.063092	-20.553438	3.706368
-13.848717	-21.239036	3.716365
-13.529262	-19.247975	3.726362
-13.626783	-15.292270	3.736358
-12.565843	-11.565652	3.746355
-11.943823	-20.963324	3.756352
-11.957790	-12.359517	3.766349
-10.958882	-20.108807	3.776346
-10.145667	-15.394494	3.786342
-10.406439	-13.623686	3.796339
-9.885662	-15.744611	3.806336
-8.910233	-19.111558	3.816333
-8.486734	-17.729085	3.826330
-8.363270	-18.719946	3.836326
-7.275359	-13.873473	3.846323
-6.911499	-18.639371	3.856320
-6.992314	-21.755748	3.866317
-6.389119	-17.004998	3.876314
-5.461431	-17.955656	3.886310
-5.207241	-17.573105	3.896307
-4.798459	-12.284916	3.906304
-4.465527	-13.080090	3.916301
-3.844037	-7.705306	3.926298
-3.455646	-3.049787	3.936294
-2.764945	11.593886	3.946291
-2.390020	21.129245	3.956288
-2.047870	34.386033	3.966285
-1.684708	51.343124	3.976282
-0.954970	68.796330	3.986278
-0.872947	87.545470	3.996275
-0.564126	117.852018	4.006272
0.000000	131.742324	4.011277
0.227887	150.037675	4.016282
0.511848	157.231549	4.021286
0.376110	160.235573	4.026291
0.596170	174.405327	4.031296
1.054875	186.048076	4.036301
0.932853	193.847717	4.041306
1.173628	194.856777	4.046310
0.874468	200.875577	4.051315
0.871305	199.322239	4.056320
0.951293	193.920151	4.061325
1.060692	190.953825	4.066330
0.995698	191.642278	4.071334
0.862260	203.310782	4.076339
0.733887	207.305967	4.081344
1.358550	206.654363	4.086349
1.019510	207.873488	4.091354
1.309902	211.719262	4.096358
1.682955	229.085163	4.101363
1.489494	225.226331	4.106368
1.372643	207.286350	4.111373
1.370869	221.533751	4.116378
1.389138	209.569266	4.121382
1.416373	207.358993	4.126387
1.111069	208.300748	4.131392
1.075394	202.293089	4.136397
1.098348	207.847860	4.141402
1.407258	216.888011	4.146406
1.644918	227.093811	4.151411
1.484661	209.695415	4.156416
1.090267	206.538477	4.161421
1.273746	222.740299	4.166426
1.560430	223.892520	4.171430
1.773927	240.014322	4.176435
1.590805	223.047852	4.181440
1.647487	208.515937	4.186445
1.382885	210.452906	4.191450
1.469607	207.955975	4.196454
1.354533	200.112843	4.201459
1.156309	212.743193	4.206464
1.728122	212.558477	4.211469
1.472822	230.776027	4.216474
1.634396	237.323257	4.221478
1.423519	231.397124	4.226483
1.436227	236.810647	4.231488
2.064616	239.471659	4.236493
1.569614	244.230065	4.241498
1.825032	226.570280	4.246502
1.322623	221.451875	4.251507
1.476191	233.094478	4.256512
1.428599	236.191581	4.261517
1.506693	249.645053	4.266522
1.946498	234.932397	4.271526
1.750079	243.549679	4.276531
1.965109	242.641788	4.281536
1.923672	229.378199	4.286541
1.974518	241.591830	4.291546
1.949099	235.072417	4.296550
1.669156	223.164801	4.301555
1.775781	205.539200	4.306560
2.040432	202.027008	4.311565
1.781831	216.611826	4.316570
1.354783	199.304393	4.321574
1.678696	221.742656	4.326579
1.592117	236.588715	4.331584
1.808104	235.830424	4.336589
1.618760	244.917122	4.341594
1.856915	242.863476	4.346598
1.644370	241.702461	4.351603
1.774903	245.083951	4.356608
1.683724	237.486251	4.361613
1.857023	239.696345	4.366618
1.790975	235.265959	4.371622
1.555789	241.872643	4.376627
1.423821	248.116289	4.381632
2.003283	254.566646	4.386637
1.838090	269.266893	4.391642
1.919998	272.784776	4.396646
1.989440	268.013431	4.401651
2.065551	276.159205	4.406656
2.009470	268.776776	4.411661
2.060352	274.222381	4.416666
1.990777	277.053895	4.421670
1.834301	268.953766	4.426675
1.868680	270.627644	4.431680
2.089045	263.874136	4.436685
1.941540	270.638299	4.441690
1.942047	276.633551	4.446694
2.347608	268.725554	4.451699
1.878268	276.487235	4.456704
2.540006	261.553491	4.461709
1.900240	266.952619	4.466714
1.994365	274.341788	4.471718
1.960531	271.939551	4.476723
1.784790	281.518977	4.481728
2.028605	280.161687	4.486733
2.152475	295.237222	4.491738
2.400071	301.900785	4.496742
2.366382	307.271982	4.501747
2.183747	321.540091	4.506752
2.341172	306.558632	4.511757
2.278293	309.475665	4.516762
2.372086	301.700566	4.521766
2.534645	313.151831	4.526771
2.320939	306.714509	4.531776
2.456170	280.278006	4.536781
2.323960	283.690397	4.541786
2.657750	270.383704	4.546790
2.383387	280.713817	4.551795
2.309834	283.178301	4.556800
2.623241	274.216797	4.561805
2.252251	291.548671	4.566810
2.305407	276.923453	4.571814
2.637180	298.326424	4.576819
2.233936	286.193484	4.581824
2.601879	290.201279	4.586829
2.312302	290.969865	4.591834
2.661029	303.950987	4.596838
2.956528	303.899541	4.601843
2.410858	286.627200	4.606848
2.805003	282.589953	4.611853
2.338330	276.396792	4.616858
2.446548	283.535814	4.621862
2.491709	282.621760	4.626867
2.287108	289.246002	4.631872
2.802694	304.236883	4.636877
2.653500	316.115647	4.641882
2.635204	310.313829	4.646886
2.957388	309.797548	4.651891
2.712458	293.435713	4.656896
2.484840	280.261450	4.661901
2.264032	291.618503	4.666906
2.189506	297.475319	4.671910
2.777297	298.983159	4.676915
2.658470	318.566637	4.681920
2.654315	312.441949	4.686925
2.447941	314.719239	4.691930
2.659505	319.702642	4.696934
2.752041	325.024276	4.701939
2.418079	314.387816	4.706944
2.688664	314.676311	4.711949
2.412543	322.554362	4.716954
2.521607	314.023102	4.721958
2.962901	319.759856	4.726963
2.697020	322.033169	4.731968
3.026141	331.468913	4.736973
2.783072	325.716863	4.741978
2.785651	334.647492	4.746982
3.017151	342.358792	4.751987
2.887070	348.619629	4.756992
3.263588	338.679056	4.761997
2.943984	327.388888	4.767002
2.808128	327.052581	4.772006
2.686870	321.224761	4.777011
2.777172	335.365696	4.782016
2.999997	337.037246	4.787021
3.020763	340.153854	4.792026
3.130911	345.966949	4.797030
3.223562	336.725995	4.802035
3.151281	342.378240	4.807040
3.268269	329.195425	4.812045
2.900456	318.690835	4.817050
3.006414	318.062797	4.822054
3.009911	318.568670	4.827059
2.926168	338.390055	4.832064
3.310310	340.878157	4.837069
2.909996	351.480507	4.842074
3.094944	337.961185	4.847078
3.284226	335.782517	4.852083
3.218627	354.970219	4.857088
2.925430	327.969686	4.862093
3.131462	342.936487	4.867098
3.235223	338.283164	4.872102
3.250791	344.159934	4.877107
3.184907	346.514738	4.882112
3.250672	331.967887	4.887117
3.056372	355.277482	4.892122
3.026339	331.767501	4.897126
3.157123	333.492442	4.902131
3.084926	350.526687	4.907136
3.201123	340.140787	4.912141
3.069179	345.068006	4.917146
3.382397	343.429910	4.922150
3.341034	334.209133	4.927155
2.956434	350.098312	4.932160
3.309906	339.904942	4.937165
3.234995	348.263652	4.942170
3.227398	337.121002	4.947174
3.214637	337.959665	4.952179
2.885840	362.022735	4.957184
3.196514	368.394832	4.962189
3.054269	379.016212	4.967194
3.142133	372.872051	4.972198
3.463140	374.140056	4.977203
3.347010	382.602279	4.982208
3.365567	380.112936	4.987213
3.270977	378.640493	4.992218
3.167248	382.702978	4.997222
3.510705	378.411856	5.002227
3.614153	383.825628	5.007232
3.878206	382.183618	5.012237
3.460596	384.138889	5.017242
3.401632	384.000997	5.022246
3.541217	385.500836	5.027251
3.293625	385.321211	5.032256
3.415164	392.100651	5.037261
3.533134	416.117793	5.042266
3.402950	409.744760	5.047270
3.635564	403.620369	5.052275
3.718676	412.349991	5.057280
3.918465	405.442367	5.062285
3.824585	416.003098	5.067290
3.620569	418.861591	5.072294
4.088823	405.175819	5.077299
3.684361	405.114066	5.082304
3.684098	398.527483	5.087309
3.553135	406.764078	5.092314
3.612696	403.215688	5.097318
4.086931	408.925919	5.102323
3.879169	421.935968	5.107328
4.141142	413.212851	5.112333
4.154428	408.799197	5.117338
4.221932	391.938120	5.122342
3.728190	390.942345	5.127347
3.338249	390.622278	5.132352
3.668037	379.225838	5.137357
3.514190	388.242529	5.142362
3.609690	403.780427	5.147366
4.232117	415.485282	5.152371
3.813915	422.494223	5.157376
4.133572	423.250726	5.162381
3.953901	422.475238	5.167386
3.909534	425.480491	5.172390
4.036467	420.889314	5.177395
3.683680	416.392018	5.182400
4.027794	412.706725	5.187405
3.964738	425.483316	5.192410
4.208623	417.629290	5.197414
3.867561	412.631548	5.202419
4.027112	419.049458	5.207424
4.134104	405.026988	5.212429
4.127300	421.140105	5.217434
3.653114	411.616606	5.222438
3.236147	410.999709	5.227443
3.518270	423.223309	5.232448
3.897816	414.770712	5.237453
4.059301	424.014213	5.242458
4.030887	413.400195	5.247462
3.957041	424.300154	5.252467
3.992328	448.259781	5.257472
4.472003	442.530804	5.262477
4.304758	449.144009	5.267482
4.033676	450.343535	5.272486
4.522569	444.396286	5.277491
4.218291	428.747239	5.282496
4.336471	419.513955	5.287501
4.315223	416.585257	5.292506
4.015088	413.844024	5.297510
4.519645	423.170821	5.302515
4.339529	425.307050	5.307520
4.091246	408.588116	5.312525
4.369776	418.583861	5.317530
4.496923	429.336660	5.322534
4.516916	418.276703	5.327539
4.039840	421.444623	5.332544
4.426394	418.362207	5.337549
4.360365	422.853843	5.342554
4.202277	419.111450	5.347558
4.426438	423.876847	5.352563
4.469790	446.487789	5.357568
4.529754	435.296512	5.362573
4.622460	437.802703	5.367578
4.134326	421.593885	5.372582
4.750856	433.604478	5.377587
4.367462	436.151465	5.382592
4.267853	423.736986	5.387597
4.451598	434.104949	5.392602
4.539867	454.526103	5.397606
4.616110	453.200536	5.402611
4.369632	459.324876	5.407616
4.499852	461.265093	5.412621
4.639777	456.814021	5.417626
4.420259	444.472124	5.422630
4.253155	458.226654	5.427635
4.369159	458.366470	5.432640
4.679563	457.158379	5.437645
4.710401	449.170645	5.442650
4.549949	450.288452	5.447654
4.804856	456.430363	5.452659
4.757244	463.071553	5.457664
4.838968	449.924849	5.462669
4.986921	461.767641	5.467674
4.546064	454.178787	5.472678
4.818889	457.153035	5.477683
4.529179	454.920816	5.482688
4.723190	454.210937	5.487693
4.794168	448.393426	5.492698
4.554686	456.706090	5.497702
4.792361	457.942196	5.502707
4.569607	452.101009	5.507712
4.948282	461.917252	5.512717
4.748612	454.992946	5.517722
4.695824	452.530772	5.522726
4.886583	455.789493	5.527731
4.832825	453.198929	5.532736
4.919249	444.761116	5.537741
4.636922	451.804836	5.542746
4.570932	448.563979	5.547750
5.144031	450.282724	5.552755
4.886838	456.334742	5.557760
4.861777	445.754676	5.562765
4.620520	450.682335	5.567770
4.857750	449.714726	5.572774
5.074791	448.963749	5.577779
4.893463	455.172721	5.582784
4.718702	457.187708	5.587789
4.766662	455.231763	5.592794
4.856767	452.726835	5.597798
5.146305	459.154257	5.602803
4.917584	469.067924	5.607808
5.184145	481.213639	5.612813
5.155217	467.539733	5.617818
4.857987	472.224088	5.622822
4.996147	465.332048	5.627827
4.911480	470.565517	5.632832
5.219638	481.394199	5.637837
5.329448	481.008410	5.642842
5.209009	481.929299	5.647846
5.287958	475.865495	5.652851
5.002118	483.435058	5.657856
4.979002	485.575834	5.662861
5.122406	477.772518	5.667866
5.038824	484.240303	5.672870
5.234114	481.912045	5.677875
5.023648	478.873724	5.682880
4.923614	481.811532	5.687885
5.008384	478.119162	5.692890
4.972666	480.807788	5.697894
5.278708	479.814796	5.702899
4.953649	483.181261	5.707904
5.166213	478.661056	5.712909
5.094746	476.684297	5.717914
5.134999	490.241015	5.722918
5.319772	495.537008	5.727923
5.299947	511.234758	5.732928
5.585084	508.985174	5.737933
5.446181	511.663333	5.742938
5.204458	499.390075	5.747942
5.440414	500.993768	5.752947
5.574223	515.403424	5.757952
5.390045	508.025771	5.762957
5.368360	505.119524	5.767962
5.312689	514.380025	5.772966
5.321951	499.756127	5.777971
5.228408	513.961349	5.782976
5.242638	514.190597	5.787981
5.111057	515.367863	5.792986
5.164304	524.265663	5.797990
5.286260	519.224318	5.802995
5.462742	516.299330	5.808000
5.661217	507.228332	5.813005
5.175069	513.586063	5.818010
5.270450	513.637932	5.823014
5.597612	524.770819	5.828019
5.473679	544.095171	5.833024
5.808200	538.003116	5.838029
5.572756	542.114542	5.843034
5.609418	541.288497	5.848038
6.039817	538.925520	5.853043
5.650593	530.158221	5.858048
5.648459	520.010872	5.863053
5.362836	513.823012	5.868058
5.725414	524.690875	5.873062
5.923693	536.380974	5.878067
5.648319	547.914555	5.883072
6.055184	533.248299	5.888077
5.550797	520.556125	5.893082
5.589757	536.073410	5.898086
6.126464	531.867020	5.903091
5.751211	538.701693	5.908096
5.763030	520.202105	5.913101
5.773210	517.297496	5.918106
5.815697	533.225002	5.923110
6.054649	534.447684	5.928115
5.649801	524.413945	5.933120
5.949984	527.503750	5.938125
5.746921	535.309656	5.943130
5.830057	540.806950	5.948134
5.952289	538.226849	5.953139
6.089286	550.684083	5.958144
6.010293	531.971886	5.963149
5.992306	524.101889	5.968154
5.975300	526.576503	5.973158
5.828413	511.615637	5.978163
5.802187	529.659438	5.983168
5.834566	536.922889	5.988173
6.037905	540.945325	5.993178
5.897363	545.787112	5.998182
6.127766	540.779436	6.003187
5.864248	551.616120	6.008192
5.975989	553.738664	6.013197
6.256417	537.841635	6.018202
5.955612	540.266665	6.023206
5.983370	543.340426	6.028211
5.943590	547.709076	6.033216
6.011419	546.982852	6.038221
6.219026	546.458467	6.043226
5.819247	545.369608	6.048230
6.087295	554.304243	6.053235
5.995714	550.188854	6.058240
6.469985	553.295179	6.063245
6.335148	540.220098	6.068250
6.353142	544.659012	6.073254
6.256674	527.165066	6.078259
5.661621	520.753186	6.083264
5.767604	523.927669	6.088269
6.097601	530.445514	6.093274
5.831808	552.082852	6.098278
6.121728	532.994380	6.103283
6.086369	549.848036	6.108288
6.047932	551.540095	6.113293
6.148201	544.188325	6.118298
5.766749	548.264193	6.123302
6.098929	539.645029	6.128307
6.092701	552.007051	6.133312
5.854162	547.379551	6.138317
5.930400	547.980158	6.143322
5.778261	554.725578	6.148326
6.364849	538.250531	6.153331
6.114768	545.034923	6.158336
6.161095	540.116665	6.163341
6.384066	550.845426	6.168346
6.071432	553.607650	6.173350
6.145133	557.413750	6.178355
5.966928	549.297431	6.183360
6.183253	540.999599	6.188365
6.467696	555.790471	6.193370
5.978072	527.762667	6.198374
6.323329	512.759536	6.203379
5.897124	514.300800	6.208384
6.060079	506.291499	6.213389
6.236070	517.859677	6.218394
5.778344	516.322038	6.223398
5.983249	501.345763	6.228403
5.926915	507.133749	6.233408
6.005779	502.478670	6.238413
5.948566	509.278034	6.243418
5.982793	521.415118	6.248422
6.340466	517.975286	6.253427
6.097892	513.065318	6.258432
6.302977	512.524085	6.263437
5.980479	516.803301	6.268442
5.735328	508.443927	6.273446
5.890806	517.200027	6.278451
6.096361	521.702649	6.283456
6.175324	520.733370	6.288461
6.063087	514.023177	6.293466
5.965483	512.318389	6.298470
6.050099	514.933761	6.303475
5.841884	512.640711	6.308480
5.934328	524.497559	6.313485
6.122706	531.685702	6.318490
6.188343	550.587559	6.323494
6.277366	538.533088	6.328499
5.833267	519.864966	6.333504
5.950296	524.847880	6.338509
6.327350	528.491470	6.343514
5.851787	530.318118	6.348518
6.361173	511.553994	6.353523
5.982168	515.120085	6.358528
5.762347	510.587370	6.363533
6.209934	516.073557	6.368538
5.950961	522.261350	6.373542
6.023433	518.017340	6.378547
5.900467	527.882984	6.383552
6.420930	531.023797	6.388557
6.227388	519.286456	6.393562
6.265707	528.102571	6.398566
6.240427	502.506429	6.403571
6.127973	514.349086	6.408576
6.386970	515.256401	6.413581
6.370934	510.824873	6.418586
6.194925	515.688099	6.423590
6.316095	510.241309	6.428595
6.049764	517.345458	6.433600
6.135212	503.352997	6.438605
6.178896	519.706193	6.443610
6.179197	520.258082	6.448614
6.124187	509.013042	6.453619
6.082279	517.243858	6.458624
5.587044	508.272113	6.463629
5.607010	522.192408	6.468634
5.747018	514.420119	6.473638
5.931553	509.845047	6.478643
5.881133	517.863086	6.483648
6.009833	519.551199	6.488653
5.956550	515.599870	6.493658
5.718080	514.705249	6.498662
6.247604	515.945121	6.503667
6.194582	516.076468	6.508672
6.016204	518.454230	6.513677
5.970325	511.278460	6.518682
5.890402	522.433042	6.523686
6.329956	515.790890	6.528691
6.086487	527.903430	6.533696
6.240835	525.262480	6.538701
6.282550	512.625780	6.543706
5.946491	522.743780	6.548710
6.540935	511.631737	6.553715
6.069649	515.930511	6.558720
5.677649	522.880314	6.563725
6.205994	508.001723	6.568730
5.888000	512.490629	6.573734
5.803459	513.695243	6.578739
5.749696	530.617033	6.583744
5.819503	521.137837	6.588749
5.736492	515.869123	6.593754
5.762634	520.751627	6.598758
5.883868	531.832720	6.603763
6.154909	545.505744	6.608768
5.659504	547.022437	6.613773
6.155086	547.572586	6.618778
5.880944	555.321386	6.623782
6.374998	548.277065	6.628787
6.347142	556.319808	6.633792
6.487291	543.858112	6.638797
6.115093	532.952664	6.643802
5.775613	533.866641	6.648806
6.027405	514.034700	6.653811
5.987822	527.056902	6.658816
6.131234	517.004778	6.663821
5.928828	514.862206	6.668826
5.767007	520.610310	6.673830
6.464327	522.446261	6.678835
6.095208	530.537199	6.683840
5.861982	525.212605	6.688845
5.996873	514.962210	6.693850
5.953145	525.312086	6.698854
6.196478	534.284929	6.703859
6.046058	531.390382	6.708864
5.896089	518.862110	6.713869
6.268119	528.839318	6.718874
6.063776	516.521196	6.723878
6.114856	522.948492	6.728883
5.987597	524.930381	6.733888
5.838008	512.784150	6.738893
6.192041	514.217583	6.743898
5.803353	507.836421	6.748902
6.096864	532.226662	6.753907
5.936383	542.979325	6.758912
6.048421	534.740956	6.763917
6.062964	537.055170	6.768922
5.902059	550.687212	6.773926
6.156115	549.488130	6.778931
6.055758	544.920567	6.783936
6.315547	551.982378	6.788941
6.208155	530.576605	6.793946
6.066555	532.224741	6.798950
6.207613	524.780703	6.803955
6.042156	519.091523	6.808960
6.203227	525.767904	6.813965
6.178221	517.341955	6.818970
5.897751	524.129091	6.823974
6.095090	515.181202	6.828979
5.880157	524.024961	6.833984
5.885131	514.939075	6.838989
6.187073	520.800058	6.843994
5.992834	520.671695	6.848998
6.198669	519.953644	6.854003
6.056388	525.192609	6.859008
6.052157	521.739973	6.864013
6.040147	523.358898	6.869018
6.135107	520.853354	6.874022
6.122708	517.945175	6.879027
6.168165	519.143204	6.884032
5.780114	517.230795	6.889037
5.926226	526.748501	6.894042
5.629183	517.079641	6.899046
6.202702	524.240733	6.904051
6.027360	523.618035	6.909056
5.935659	519.365640	6.914061
6.268743	520.246407	6.919066
5.818257	527.563410	6.924070
6.259143	527.534602	6.929075
6.223736	518.882473	6.934080
6.131574	517.884747	6.939085
6.236218	512.217525	6.944090
5.781762	524.910601	6.949094
6.020756	511.041534	6.954099
6.097645	509.057222	6.959104
6.008922	515.319973	6.964109
6.114248	513.414623	6.969114
5.911355	520.322617	6.974118
6.115697	512.915284	6.979123
6.005468	521.067714	6.984128
5.966297	523.232852	6.989133
6.286642	520.074935	6.994138
6.093900	519.596291	6.999142
6.090406	525.258347	7.004147
5.908551	518.516840	7.009152
6.103817	523.580744	7.014157
6.036053	519.510066	7.019162
6.033016	523.521122	7.024166
5.974529	517.863987	7.029171
5.870006	510.337615	7.034176
5.982013	516.533354	7.039181
6.224085	523.899575	7.044186
5.875387	531.106823	7.049190
6.017434	518.645129	7.054195
6.038000	522.064881	7.059200
6.179737	533.735219	7.064205
5.848356	519.820410	7.069210
5.975606	532.975758	7.074214
6.101136	549.058852	7.079219
6.142969	547.752776	7.084224
6.079047	541.378603	7.089229
5.938832	525.581489	7.094234
5.709058	549.557947	7.099238
6.348656	549.005086	7.104243
6.339222	544.802821	7.109248
6.000688	540.445100	7.114253
6.105581	526.725744	7.119258
5.975451	525.064904	7.124262
5.921755	516.944205	7.129267
5.988240	534.881335	7.134272
6.004177	547.871786	7.139277
6.377309	544.028254	7.144282
6.032882	542.525458	7.149286
6.222014	524.590873	7.154291
5.855094	526.473559	7.159296
5.894384	523.265010	7.164301
5.987292	524.827232	7.169306
5.828182	541.815674	7.174310
6.036488	543.747931	7.179315
6.086234	550.916768	7.184320
6.307546	548.171714	7.189325
6.198872	539.899179	7.194330
5.834180	532.971230	7.199334
5.875212	537.355527	7.204339
6.205830	544.530331	7.209344
6.188105	547.135984	7.214349
6.377156	528.043864	7.219354
6.080560	528.249205	7.224358
5.960972	524.043050	7.229363
5.866273	524.652470	7.234368
6.006630	527.223412	7.239373
6.071499	534.178419	7.244378
5.864708	526.210875	7.249382
6.190735	531.708573	7.254387
6.089032	537.814345	7.259392
5.533127	536.037308	7.264397
5.878275	525.993177	7.269402
6.168872	547.763103	7.274406
6.215941	549.396044	7.279411
6.235694	555.007309	7.284416
6.080535	545.864799	7.289421
6.322066	536.144806	7.294426
5.983471	529.962931	7.299430
5.996941	524.630618	7.304435
6.085347	522.781140	7.309440
5.784657	525.033993	7.314445
6.387873	530.044293	7.319450
5.902018	527.643514	7.324454
6.315980	516.291271	7.329459
6.040170	524.649536	7.334464
5.779387	523.670600	7.339469
6.149829	520.064887	7.344474
5.949650	515.508108	7.349478
6.087414	519.767299	7.354483
6.063862	512.336955	7.359488
5.683325	520.784348	7.364493
6.280322	540.012343	7.369498
6.027636	544.030428	7.374502
5.975586	528.299640	7.379507
6.259642	529.287167	7.384512
5.911890	536.658723	7.389517
5.971802	532.260413	7.394522
6.054222	553.870891	7.399526
5.974977	544.174110	7.404531
6.425214	551.718943	7.409536
5.754032	550.985904	7.414541
5.933604	535.385633	7.419546
6.218874	541.247109	7.424550
6.420601	550.590191	7.429555
5.958028	527.620606	7.434560
5.563217	521.884779	7.439565
6.064023	536.260540	7.444570
5.916445	548.246259	7.449574
6.393424	551.084874	7.454579
6.248160	544.855949	7.459584
5.915007	528.829571	7.464589
6.034823	517.118189	7.469594
5.771533	526.331419	7.474598
5.772130	539.225248	7.479603
6.077431	547.988373	7.484608
6.029201	559.723865	7.489613
6.528758	552.652094	7.494618
6.143300	560.561458	7.499622
5.911147	534.746394	7.504627
6.216455	536.465503	7.509632
5.998871	541.653580	7.514637
6.075062	524.740804	7.519642
5.803529	533.973553	7.524646
6.293368	533.953131	7.529651
5.972214	539.393324	7.534656
6.088158	532.271405	7.539661
6.256057	517.410049	7.544666
5.690424	527.175211	7.549670
5.763397	524.410182	7.554675
6.386385	546.464752	7.559680
6.059064	545.261612	7.564685
6.220005	534.229382	7.569690
5.965273	532.713540	7.574694
5.856153	521.280712	7.579699
5.468257	535.762496	7.584704
5.942871	548.897152	7.589709
6.443006	547.024221	7.594714
6.017167	563.040007	7.599718
6.187118	546.349476	7.604723
6.632686	549.778515	7.609728
6.168921	541.084991	7.614733
6.355004	526.810886	7.619738
6.111654	531.070219	7.624742
5.880616	525.309002	7.629747
5.782232	518.392692	7.634752
5.467047	528.859254	7.639757
5.866127	537.175843	7.644762
6.221201	557.495722	7.649766
6.409017	554.343519	7.654771
5.902633	551.073409	7.659776
5.696678	537.682147	7.664781
6.088743	555.989720	7.669786
6.161020	554.599390	7.674790
6.320869	553.534265	7.679795
6.262329	544.119970	7.684800
5.899129	533.652848	7.689805
6.202013	529.772488	7.694810
6.148299	521.360062	7.699814
6.011680	517.061125	7.704819
6.235789	513.593644	7.709824
6.004613	531.063294	7.714829
6.100036	522.419633	7.719834
5.971856	520.361772	7.724838
5.937325	523.489726	7.729843
5.828310	531.403310	7.734848
6.061552	529.445543	7.739853
6.259779	528.743843	7.744858
6.134908	530.305060	7.749862
6.011086	528.999034	7.754867
6.193981	521.791963	7.759872
5.805932	543.859118	7.764877
6.132757	527.684704	7.769882
5.810131	529.920760	7.774886
5.767537	527.041247	7.779891
5.978028	541.969424	7.784896
6.088134	548.487310	7.789901
6.456635	550.061705	7.794906
6.071724	552.345350	7.799910
6.161622	541.522663	7.804915
6.327262	537.439058	7.809920
5.806310	532.581403	7.814925
5.904924	541.165582	7.819930
6.061617	535.290069	7.824934
5.949511	532.217527	7.829939
5.970694	539.819250	7.834944
6.056265	546.102144	7.839949
6.119278	531.250413	7.844954
6.251943	533.644354	7.849958
6.145285	537.346575	7.854963
6.053986	540.478488	7.859968
5.827334	539.901758	7.864973
6.026659	532.740014	7.869978
6.053871	531.524949	7.874982
5.784284	532.694933	7.879987
6.409497	536.349704	7.884992
6.259285	533.141690	7.889997
6.240976	531.834307	7.895002
5.806552	531.763001	7.900006
5.933555	536.340368	7.905011
6.110151	524.928886	7.910016
6.202532	538.799245	7.915021
6.290659	531.938727	7.920026
6.083972	537.562250	7.925030
6.108904	528.292417	7.930035
5.957834	529.581526	7.935040
5.679732	544.930917	7.940045
6.318674	534.178705	7.945050
5.948080	532.036203	7.950054
5.838546	537.857854	7.955059
6.007104	524.555853	7.960064
6.129356	539.209546	7.965069
6.269537	541.406510	7.970074
5.931226	535.434825	7.975078
5.949007	532.522248	7.980083
6.002686	530.213833	7.985088
6.151685	540.153125	7.990093
6.210983	524.215801	7.995098
6.186303	531.283177	8.000102
5.997425	527.188807	8.005107
6.054807	529.182210	8.010112
5.912741	531.574440	8.015130
5.976760	532.863847	8.020147
6.165397	536.691199	8.025165
5.846730	542.792203	8.030182
6.197825	537.430186	8.035200
6.077905	538.359618	8.040218
6.201389	531.194546	8.045235
5.971977	536.325675	8.050253
6.162033	536.090523	8.055270
5.800256	534.158148	8.060288
5.760283	539.290347	8.065306
5.880335	533.817232	8.070323
5.913025	560.570377	8.075341
6.007525	567.022121	8.080358
6.303446	564.251373	8.085376
6.026200	565.317414	8.090394
6.342798	570.125198	8.095411
5.929452	570.425504	8.100429
6.225252	566.241771	8.105446
6.219576	570.756427	8.110464
6.397916	569.137069	8.115482
6.239658	557.990513	8.120499
6.125865	561.116327	8.125517
6.204638	565.245545	8.130534
6.271744	557.393264	8.135552
6.021713	552.945676	8.140570
5.986035	555.397493	8.145587
6.173857	557.589289	8.150605
6.070974	564.277449	8.155622
6.665768	555.159656	8.160640
6.032614	563.518891	8.165658
6.081407	555.028427	8.170675
6.232393	566.789947	8.175693
6.185710	563.591663	8.180710
6.231191	563.309846	8.185728
6.260332	568.968813	8.190746
6.200243	564.396642	8.195763
6.249520	568.886963	8.200781
6.083948	563.719256	8.205798
6.253050	563.339170	8.210816
6.092792	564.472868	8.215834
6.414566	561.437763	8.220851
6.407060	570.638496	8.225869
6.419685	554.121266	8.230886
6.479138	555.951381	8.235904
6.323963	557.673392	8.240922
5.982733	555.225812	8.245939
6.199795	556.807287	8.250957
6.112348	557.966542	8.255974
6.130335	562.347193	8.260992
6.239070	559.350838	8.266010
6.679478	557.717399	8.271027
6.276591	556.838258	8.276045
6.055602	562.284083	8.281062
6.036877	562.012876	8.286080
5.730206	570.349355	8.291098
6.259422	563.001000	8.296115
6.432719	556.902075	8.301133
6.110375	557.411705	8.306150
6.518775	563.134346	8.311168
6.341548	560.636438	8.316186
6.578965	556.572177	8.321203
6.220291	557.271239	8.326221
6.138804	561.520327	8.331238
6.449478	555.850479	8.336256
6.345947	561.606354	8.341274
6.494245	552.883644	8.346291
6.236237	556.693690	8.351309
6.438570	547.742510	8.356326
6.482811	559.225858	8.361344
6.421198	559.513794	8.366362
6.046589	566.818695	8.371379
6.358940	565.942294	8.376397
6.391432	568.117939	8.381414
6.531048	563.300307	8.386432
6.395238	571.083655	8.391450
6.217718	554.040282	8.396467
6.508681	568.349218	8.401485
6.567209	581.147871	8.406502
6.228044	561.537429	8.411520
6.445065	588.694718	8.416538
6.953818	590.029311	8.421555
6.678175	574.314174	8.426573
6.284708	561.075612	8.431590
6.787666	566.724667	8.436608
6.384154	562.645876	8.441626
6.169663	566.857214	8.446643
6.553823	560.511573	8.451661
6.283048	557.513087	8.456678
6.506187	570.617828	8.461696
6.374015	594.574136	8.466714
6.514379	583.202261	8.471731
6.569674	594.201522	8.476749
6.658590	604.012201	8.481766
6.649184	587.387968	8.486784
6.908272	596.733992	8.491802
6.400354	592.980260	8.496819
6.632669	566.666247	8.501837
6.200535	571.194206	8.506854
6.569467	581.860285	8.511872
6.508442	599.116707	8.516890
6.634608	606.386693	8.521907
6.556677	594.084541	8.526925
6.346198	606.568196	8.531942
6.716752	594.686022	8.536960
6.619800	599.404316	8.541978
6.472379	594.799432	8.546995
6.752193	599.849577	8.552013
6.403993	596.799521	8.557030
6.624211	602.529068	8.562048
6.294038	601.824879	8.567066
6.256234	600.482038	8.572083
6.940480	595.200842	8.577101
6.522796	596.967912	8.582119
6.709485	600.239905	8.587136
6.547739	599.799359	8.592154
6.286789	596.585111	8.597171
6.579138	604.648435	8.602189
6.296686	598.293873	8.607207
6.268290	598.962563	8.612224
6.356536	602.770997	8.617242
6.589848	615.451737	8.622259
6.875718	623.763731	8.627277
6.621868	626.376688	8.632295
6.943096	618.749551	8.637312
7.038171	622.418011	8.642330
6.743305	611.909225	8.647347
6.922872	608.112235	8.652365
6.735113	603.392877	8.657383
6.805989	598.120545	8.662400
7.045628	592.921486	8.667418
6.770514	602.875870	8.672435
6.963385	588.808148	8.677453
6.596857	600.131897	8.682471
6.547192	602.090461	8.687488
7.030239	595.810338	8.692506
6.666042	590.844803	8.697523
6.906443	592.783771	8.702541
6.595753	606.890361	8.707559
6.822809	594.604230	8.712576
6.964945	598.726430	8.717594
6.634702	604.187471	8.722611
6.802468	594.988877	8.727629
6.468143	604.721105	8.732647
6.624413	596.356038	8.737664
6.782770	602.689785	8.742682
6.876317	621.431116	8.747699
7.004052	616.436234	8.752717
6.783693	618.056841	8.757735
6.839439	602.221766	8.762752
6.945242	598.245275	8.767770
6.899866	605.504740	8.772787
7.117809	599.374705	8.777805
6.860126	594.718372	8.782823
6.952053	595.501894	8.787840
7.136280	600.590469	8.792858
6.881221	598.336474	8.797875
7.019050	593.038219	8.802893
6.832851	599.987556	8.807911
6.733159	598.013041	8.812928
6.827079	595.777048	8.817946
6.929550	599.082935	8.822963
7.280408	602.693964	8.827981
6.962500	605.091663	8.832999
7.116296	596.011496	8.838016
7.103171	603.200879	8.843034
6.954859	601.220917	8.848051
6.764089	600.746299	8.853069
7.249968	607.396910	8.858087
7.044173	599.387779	8.863104
6.998241	596.965884	8.868122
6.957249	597.582335	8.873139
7.376041	596.171122	8.878157
6.951079	596.207356	8.883175
6.740468	603.469919	8.888192
7.059288	600.128761	8.893210
6.782349	603.280463	8.898227
7.263392	598.443102	8.903245
7.134937	602.734012	8.908263
6.818525	595.530803	8.913280
7.144587	596.844908	8.918298
7.106479	601.383729	8.923315
7.275597	592.050983	8.928333
7.148316	609.553457	8.933351
7.038198	602.645516	8.938368
7.233771	602.025274	8.943386
7.202055	605.490712	8.948403
7.300431	594.590539	8.953421
6.956462	606.176849	8.958439
7.189329	608.050246	8.963456
7.122377	598.249425	8.968474
6.824831	600.412209	8.973491
7.091648	588.479185	8.978509
6.983058	596.796424	8.983527
7.403522	600.826377	8.988544
7.190524	597.671120	8.993562
6.696546	605.963390	8.998579
7.103492	602.088282	9.003597
7.077709	604.219440	9.008615
7.313451	604.287599	9.013632
7.261980	601.009308	9.018650
7.108323	608.723001	9.023667
7.367483	595.954984	9.028685
7.167720	598.260435	9.033703
7.059310	606.306050	9.038720
7.436960	594.516878	9.043738
7.068747	593.403605	9.048755
7.258068	606.401782	9.053773
7.185896	598.767734	9.058791
6.831412	606.513729	9.063808
7.347441	605.753242	9.068826
6.960333	599.781651	9.073843
7.033729	599.302443	9.078861
6.978752	603.568319	9.083879
7.144854	598.485819	9.088896
7.634052	594.687948	9.093914
7.215479	598.438336	9.098931
7.616328	605.716460	9.103949
7.480265	600.486888	9.108967
7.166648	603.718456	9.113984
7.197875	601.751532	9.119002
7.173706	596.333424	9.124019
7.596744	596.462640	9.129037
7.173262	604.142689	9.134055
7.313665	605.468584	9.139072
7.237830	596.049668	9.144090
7.339339	610.062556	9.149107
7.214591	596.938086	9.154125
7.014225	595.054801	9.159143
7.022757	612.804170	9.164160
7.456834	609.602592	9.169178
7.139907	604.453488	9.174195
7.664676	595.874009	9.179213
7.616992	598.977098	9.184231
7.257400	603.617168	9.189248
7.294473	604.274645	9.194266
7.393165	601.505389	9.199283
7.493557	595.841937	9.204301
7.307122	602.510857	9.209319
7.068144	605.551977	9.214336
7.098453	597.322564	9.219354
7.361897	624.624774	9.224371
7.557333	631.229320	9.229389
7.614565	621.434530	9.234407
7.137938	624.484225	9.239424
7.441137	618.022930	9.244442
7.507772	632.570730	9.249459
7.669063	630.313757	9.254477
7.469961	623.645764	9.259495
7.310125	625.412639	9.264512
7.745952	626.896169	9.269530
7.473407	623.707744	9.274547
7.649160	614.846039	9.279565
7.489705	598.176625	9.284583
7.448862	595.379456	9.289600
7.370949	606.011545	9.294618
7.319300	611.295176	9.299635
7.464277	621.637144	9.304653
7.916694	627.962652	9.309671
7.473827	620.362990	9.314688
7.699518	618.120667	9.319706
7.384001	614.981069	9.324723
7.594028	606.493945	9.329741
7.444299	610.169105	9.334759
7.464331	627.078271	9.339776
7.704762	628.655597	9.344794
7.560997	632.542629	9.349811
7.638014	630.723024	9.354829
7.559711	630.146960	9.359847
7.275425	639.646379	9.364864
7.814355	630.022618	9.369882
7.559348	634.067180	9.374899
7.730484	622.953525	9.379917
7.902376	629.828345	9.384935
7.324369	626.384949	9.389952
7.551979	613.580604	9.394970
7.446218	625.265725	9.399987
7.399582	623.271811	9.405005
7.758734	629.305804	9.410023
7.375784	627.238951	9.415040
7.812372	618.957342	9.420058
7.819381	625.301153	9.425075
7.784423	617.732585	9.430093
7.673286	624.807198	9.435111
7.351464	628.988859	9.440128
7.498603	625.210017	9.445146
7.782391	627.431427	9.450163
7.806688	625.758304	9.455181
8.015655	630.997002	9.460199
7.772433	633.449771	9.465216
7.947367	626.469323	9.470234
7.622038	624.800250	9.475251
7.728642	631.093162	9.480269
7.662249	627.141774	9.485287
7.410086	638.040332	9.490304
7.473199	634.324381	9.495322
7.573106	631.947853	9.500339
7.633311	636.464926	9.505357
7.666103	627.024792	9.510375
7.228707	636.013495	9.515392
7.467707	635.930457	9.520410
8.012804	654.916238	9.525427
7.911603	660.329803	9.530445
8.294095	652.369065	9.535463
7.746347	654.423037	9.540480
7.582984	632.192813	9.545498
7.740221	638.310661	9.550515
7.781479	650.487938	9.555533
8.051905	649.353946	9.560551
7.415643	638.495832	9.565568
7.926894	653.907393	9.570586
7.925324	665.915024	9.575603
7.924683	658.972532	9.580621
8.104475	662.490708	9.585639
7.893285	667.438984	9.590656
8.211760	663.667145	9.595674
7.975132	643.052738	9.600691
7.860148	641.284249	9.605709
7.526274	635.980289	9.610727
7.616273	653.079751	9.615744
7.822528	667.848459	9.620762
7.850697	664.775553	9.625779
7.564322	669.784768	9.630797
8.275242	664.596760	9.635815
7.942714	658.846002	9.640832
7.878631	669.573272	9.645850
8.154735	669.723131	9.650867
7.910797	663.374674	9.655885
7.839173	670.857068	9.660903
7.739302	668.195994	9.665920
8.247022	661.850164	9.670938
8.140609	659.216250	9.675955
7.919352	659.961294	9.680973
8.128976	660.058077	9.685991
7.933406	666.534970	9.691008
7.915934	657.347467	9.696026
8.267489	665.964808	9.701043
7.919773	653.564996	9.706061
8.040045	663.387654	9.711079
8.007199	670.478576	9.716096
8.239853	656.092762	9.721114
8.486394	653.196918	9.726131
8.321503	662.940938	9.731149
8.192440	661.774559	9.736167
8.041696	669.858594	9.741184
7.917244	660.111223	9.746202
8.448988	659.145322	9.751219
7.854973	663.369614	9.756237
7.953537	662.709113	9.761255
7.714877	668.455279	9.766272
7.858646	655.115058	9.771290
8.346347	667.938312	9.776307
8.007537	671.705353	9.781325
7.995346	660.576602	9.786343
8.173454	670.473548	9.791360
8.147137	667.671505	9.796378
8.189262	663.545610	9.801395
7.993109	664.525534	9.806413
8.360079	666.050658	9.811431
8.071701	668.354232	9.816448
8.018145	665.363913	9.821466
8.141573	661.154616	9.826483
8.034962	666.792558	9.831501
8.326082	677.040741	9.836519
8.391172	693.929544	9.841536
8.221365	691.030367	9.846554
8.378906	682.975022	9.851571
7.920591	689.212822	9.856589
8.386289	683.709988	9.861607
8.553738	687.432238	9.866624
8.358752	687.920136	9.871642
8.291973	675.941210	9.876659
7.949630	674.856228	9.881677
8.356560	683.767814	9.886695
8.223646	692.582042	9.891712
7.964170	692.872468	9.896730
8.288655	691.794192	9.901747
8.229935	690.249129	9.906765
8.342034	685.346261	9.911783
8.495707	699.417624	9.916800
8.633345	696.641619	9.921818
8.690261	686.050635	9.926835
8.266525	689.966433	9.931853
8.569644	690.006927	9.936871
8.792567	693.554688	9.941888
8.322301	691.747583	9.946906
8.578885	679.374631	9.951923
8.269435	682.350458	9.956941
8.139880	675.230876	9.961959
8.714767	700.429588	9.966976
8.803225	702.963355	9.971994
8.621688	670.954289	9.977011
8.415582	673.938326	9.982029
8.449517	657.026299	9.987047
8.198676	659.222408	9.992064
8.110093	673.264800	9.997082
8.587555	672.899684	10.002099
8.548310	690.643459	10.007117
8.832389	688.598129	10.012135
8.486206	678.339070	10.017152
8.252365	672.000258	10.022170
8.704152	678.964646	10.027187
8.418363	688.505772	10.032205
8.744555	682.291095	10.037223
8.581934	684.768536	10.042240
8.229505	686.526800	10.047258
8.650886	681.835172	10.052275
8.218165	685.330783	10.057293
8.730886	687.036999	10.062311
8.338861	689.468609	10.067328
8.328935	695.957838	10.072346
8.547174	696.715570	10.077363
8.818724	693.560221	10.082381
8.486165	698.060740	10.087399
8.490042	693.841571	10.092416
8.495045	688.872656	10.097434
8.252032	687.819871	10.102451
8.119243	701.866544	10.107469
8.527339	692.426441	10.112487
8.468515	689.445058	10.117504
8.522520	695.702799	10.122522
8.903406	699.106271	10.127539
8.290898	701.369634	10.132557
8.723706	716.041216	10.137575
8.950643	716.377414	10.142592
8.817933	712.124819	10.147610
8.785531	703.873338	10.152627
8.595916	701.325496	10.157645
8.375105	690.871333	10.162663
8.676655	708.916811	10.167680
8.525782	728.356611	10.172698
8.880598	724.061035	10.177715
8.717640	732.151550	10.182733
8.920275	731.675975	10.187751
8.660599	729.398221	10.192768
8.285167	736.986552	10.197786
8.539724	721.308129	10.202803
8.717896	725.686464	10.207821
8.638598	730.124767	10.212839
9.038869	725.845001	10.217856
8.608442	731.606153	10.222874
8.940042	728.360081	10.227891
8.702616	736.380932	10.232909
8.547392	725.418560	10.237927
8.720623	735.051739	10.242944
8.597982	734.359497	10.247962
8.750162	723.584174	10.252979
8.704907	734.487182	10.257997
8.662789	742.868598	10.263015
9.110526	752.463311	10.268032
8.974507	755.456053	10.273050
9.452092	755.546538	10.278067
8.822066	734.596703	10.283085
9.005121	738.911845	10.288103
8.990885	730.563566	10.293120
8.605882	724.267722	10.298138
8.875508	722.752925	10.303155
8.673338	730.935927	10.308173
8.820997	753.799093	10.313191
9.517103	751.610088	10.318208
9.146402	745.649406	10.323226
8.810307	732.224378	10.328243
8.880091	735.305720	10.333261
9.136917	747.125364	10.338279
8.961317	741.839297	10.343296
8.689413	744.374465	10.348314
9.252497	748.869280	10.353331
9.285754	755.309477	10.358349
9.018505	738.034121	10.363367
9.420667	722.917019	10.368384
9.243604	726.227306	10.373402
8.919212	720.265378	10.378419
9.146893	717.562268	10.383437
8.953681	723.972370	10.388455
8.966863	718.410573	10.393472
8.937075	725.332936	10.398490
9.115778	724.123169	10.403507
9.444277	724.302847	10.408525
9.108188	725.219499	10.413543
8.668027	722.765313	10.418560
8.945769	737.656992	10.423578
9.510654	751.542161	10.428595
9.222788	741.904209	10.433613
8.781758	740.127594	10.438631
9.082388	747.448624	10.443648
9.676110	742.519086	10.448666
9.576472	756.407997	10.453683
9.477156	737.277378	10.458701
9.620913	726.507479	10.463719
9.576202	719.364901	10.468736
9.212078	734.373477	10.473754
9.257852	732.372740	10.478771
9.360266	722.052801	10.483789
9.275104	731.230349	10.488807
9.465413	721.046644	10.493824
9.182454	731.720283	10.498842
9.215657	723.572200	10.503859
9.210056	724.144428	10.508877
9.143813	734.317776	10.513895
9.641706	717.670676	10.518912
9.083103	727.874609	10.523930
9.412478	717.158179	10.528947
9.398053	721.213094	10.533965
9.223229	722.406975	10.538983
9.380509	715.704254	10.544000
8.969359	728.294680	10.549018
9.398703	729.080999	10.554035
9.238651	722.562090	10.559053
9.331303	730.860118	10.564071
9.348107	721.724578	10.569088
9.250749	733.753602	10.574106
9.114438	718.691443	10.579123
9.288077	731.214357	10.584141
9.336571	726.049303	10.589159
9.472087	728.722020	10.594176
9.097517	726.073269	10.599194
9.504987	735.125025	10.604211
9.708193	742.078071	10.609229
9.328814	733.956933	10.614247
9.692014	719.511206	10.619264
9.333825	717.874221	10.624282
9.455909	719.849487	10.629299
9.493446	713.745678	10.634317
9.191838	721.419322	10.639335
9.707794	741.828064	10.644352
9.405367	750.424322	10.649370
9.797866	743.571320	10.654387
9.604797	742.747733	10.659405
9.402786	740.482490	10.664423
9.641540	737.268489	10.669440
9.485993	734.448920	10.674458
9.435712	737.976302	10.679475
9.712784	744.635798	10.684493
9.567526	758.119433	10.689511
9.915833	737.854999	10.694528
9.290342	740.967105	10.699546
9.402530	749.324797	10.704563
9.923886	751.348038	10.709581
9.776025	758.569798	10.714599
9.965368	738.050781	10.719616
9.645742	733.796596	10.724634
9.775224	725.837875	10.729651
9.647611	723.430345	10.734669
9.188884	732.838888	10.739687
9.982749	725.411393	10.744704
9.644726	731.490281	10.749722
9.687020	731.892421	10.754739
9.608074	717.617581	10.759757
9.746580	736.172425	10.764775
9.560537	725.977895	10.769792
9.403782	735.514258	10.774810
9.886114	746.910488	10.779827
9.749553	751.362492	10.784845
9.785134	758.747011	10.789863
10.258425	756.415825	10.794880
9.985691	738.838184	10.799898
9.611034	730.259071	10.804915
9.752461	728.759850	10.809933
9.569937	724.715249	10.814951
9.396800	732.601974	10.819968
9.816904	753.448244	10.824986
9.701404	765.856205	10.830003
10.007311	758.167863	10.835021
9.936255	766.382946	10.840039
9.805966	761.331169	10.845056
9.642223	762.319126	10.850074
9.709341	764.654695	10.855091
9.713329	758.992551	10.860109
9.595555	758.578980	10.865127
9.732817	754.780384	10.870144
9.773016	764.097342	10.875162
9.682896	763.563080	10.880179
9.835149	755.549312	10.885197
9.579240	763.826334	10.890215
9.695291	749.109376	10.895232
9.692219	770.408307	10.900250
9.986251	783.902718	10.905267
10.563043	788.044164	10.910285
9.972547	772.574818	10.915303
10.059631	763.795188	10.920320
10.043156	758.201079	10.925338
9.920168	753.887035	10.930355
10.058563	750.923726	10.935373
9.925741	755.131951	10.940391
10.130727	750.776892	10.945408
10.281888	759.407132	10.950426
10.228734	755.487474	10.955443
10.375411	751.137131	10.960461
9.944165	757.815775	10.965479
9.996345	757.908465	10.970496
10.252651	752.977315	10.975514
10.304576	752.820783	10.980531
10.442240	748.731429	10.985549
10.041977	747.373292	10.990567
10.115538	750.472808	10.995584
10.127285	757.292277	11.000602
9.856652	748.332447	11.005619
10.154054	758.633376	11.010637
9.987304	751.418350	11.015655
9.854757	763.821155	11.020672
9.895917	756.692808	11.025690
9.984862	759.763607	11.030707
10.327296	762.112131	11.035725
10.105613	762.225085	11.040743
10.213944	767.178648	11.045760
10.278165	771.353822	11.050778
10.348410	777.244906	11.055795
10.569538	768.844621	11.060813
10.351799	758.198012	11.065831
9.954628	756.621392	11.070848
10.099480	757.587478	11.075866
10.090107	776.951898	11.080883
10.539197	780.353269	11.085901
10.558215	781.578297	11.090919
10.360815	769.773710	11.095936
10.185034	752.323804	11.100954
10.365547	762.087464	11.105971
10.396276	755.135218	11.110989
10.182900	754.779859	11.116007
10.182320	750.935553	11.121024
10.479751	766.296753	11.126042
10.606721	770.756876	11.131059
10.320726	757.324136	11.136077
10.290295	766.176872	11.141095
10.200229	763.329353	11.146112
10.477742	783.673246	11.151130
10.405842	793.486217	11.156147
10.583053	791.350879	11.161165
10.448205	786.190222	11.166183
10.382956	782.098474	11.171200
10.570997	791.618434	11.176218
10.336674	780.265824	11.181235
10.227562	781.079233	11.186253
10.213041	789.108541	11.191271
10.089191	780.679648	11.196288
10.168865	784.084402	11.201306
10.037460	787.422387	11.206323
10.512338	794.169271	11.211341
10.406272	789.730198	11.216359
10.100302	788.383536	11.221376
10.697021	789.761473	11.226394
10.435483	782.965565	11.231411
10.647707	792.521975	11.236429
10.477225	794.788764	11.241447
10.580880	803.958079	11.246464
10.537677	804.416174	11.251482
10.341729	821.985246	11.256499
10.773840	807.102733	11.261517
10.954149	817.813335	11.266535
10.758112	814.787194	11.271552
10.610290	791.651581	11.276570
10.250063	794.056106	11.281587
10.813994	801.418868	11.286605
10.712939	811.395006	11.291623
10.743897	815.896004	11.296640
10.950707	814.201850	11.301658
10.722561	812.304530	11.306675
10.700555	781.602483	11.311693
10.853212	797.852341	11.316711
10.589402	792.586246	11.321728
10.713074	787.372828	11.326746
10.736799	796.773910	11.331763
10.847156	804.080455	11.336781
10.319368	801.076373	11.341799
10.726687	804.302205	11.346816
11.020124	811.682022	11.351834
10.949236	818.367662	11.356851
10.956607	811.405867	11.361869
11.117379	816.954901	11.366887
11.205786	804.577167	11.371904
10.811824	787.291895	11.376922
10.856388	797.330656	11.381939
10.685411	779.616981	11.386957
10.517050	779.946475	11.391975
10.687330	795.965606	11.396992
11.160738	800.157894	11.402010
10.783478	817.524881	11.407027
11.287357	809.675277	11.412045
11.137673	801.798079	11.417063
10.951211	796.702434	11.422080
11.155655	786.154213	11.427098
10.664187	791.266639	11.432115
10.869476	788.049203	11.437133
10.700727	788.965857	11.442151
10.722503	796.535318	11.447168
11.273181	806.440748	11.452186
11.032112	807.220465	11.457203
11.159833	802.251210	11.462221
11.202243	797.375174	11.467239
11.043742	790.735627	11.472256
11.052129	783.829375	11.477274
10.999390	791.081682	11.482291
10.929888	784.184464	11.487309
11.202052	789.352941	11.492327
11.077973	789.563327	11.497344
10.871302	780.642013	11.502362
10.656896	798.113340	11.507379
10.885660	803.976958	11.512397
10.960130	820.051213	11.517415
10.865212	823.598195	11.522432
11.222236	818.195246	11.527450
11.410064	824.849450	11.532467
11.341922	818.443044	11.537485
11.286848	821.259951	11.542503
11.173095	824.640490	11.547520
11.308993	817.805948	11.552538
11.034271	822.693329	11.557555
11.313931	821.925743	11.562573
11.103114	818.011163	11.567591
10.753608	818.523223	11.572608
10.994854	819.827059	11.577626
11.015080	824.004991	11.582643
11.083826	817.496942	11.587661
11.478679	814.417828	11.592679
10.954822	824.590299	11.597696
11.421244	816.724838	11.602714
11.257783	819.515472	11.607731
11.118895	825.259575	11.612749
11.405888	817.528471	11.617767
11.363407	824.864909	11.622784
11.411528	821.223424	11.627802
11.106984	820.903599	11.632819
11.293436	826.772939	11.637837
11.095899	818.363779	11.642855
11.461398	840.624250	11.647872
11.706453	840.623758	11.652890
11.218772	825.644558	11.657907
11.666082	828.558331	11.662925
11.682129	817.700241	11.667943
11.492127	822.113666	11.672960
11.648669	804.411868	11.677978
11.598201	818.109769	11.682995
11.010765	813.945776	11.688013
11.575429	816.056241	11.693031
11.337013	817.281304	11.698048
11.773281	813.644462	11.703066
11.461386	813.298298	11.708083
11.401264	823.126563	11.713101
11.694706	818.700874	11.718119
11.382363	815.206444	11.723136
11.470565	828.017128	11.728154
11.480147	831.419306	11.733171
11.565100	831.609712	11.738189
11.927165	840.895371	11.743207
11.573650	833.446160	11.748224
11.880525	818.555598	11.753242
11.561860	816.347410	11.758259
11.612386	821.499781	11.763277
11.497662	814.869719	11.768295
11.264727	823.737257	11.773312
11.847401	823.755563	11.778330
11.826021	833.245898	11.783347
11.617603	825.057785	11.788365
11.820115	822.860791	11.793383
11.938090	826.598828	11.798400
11.922043	813.657452	11.803418
11.998606	814.123111	11.808435
11.597747	814.620827	11.813453
11.820891	813.374974	11.818471
11.910791	814.363234	11.823488
11.688885	815.128368	11.828506
10.969754	814.043353	11.833523
11.386932	809.349035	11.838541
11.643982	828.806867	11.843559
11.431948	846.828643	11.848576
11.802586	849.185214	11.853594
11.739168	851.567364	11.858611
11.767675	847.663808	11.863629
11.972089	851.832565	11.868647
11.836860	848.523189	11.873664
11.997251	832.964919	11.878682
11.888679	847.311505	11.883699
11.793376	849.526515	11.888717
12.186271	833.469570	11.893735
11.890228	850.567019	11.898752
11.692282	843.096325	11.903770
11.999218	847.885621	11.908787
11.681654	846.243187	11.913805
12.021792	838.998967	11.918823
11.772214	845.653727	11.923840
12.117354	840.080030	11.928858
12.211805	845.972848	11.933875
12.263988	846.701545	11.938893
12.321569	840.845115	11.943911
11.933849	854.921854	11.948928
11.939706	844.194442	11.953946
11.939744	847.066507	11.958963
11.930597	843.444911	11.963981
12.511159	838.374139	11.968999
12.128330	846.953330	11.974016
12.269749	838.771753	11.979034
12.212115	846.423346	11.984051
11.911399	845.085848	11.989069
12.295363	841.923798	11.994087
11.890892	848.212594	11.999104
12.055734	838.028199	12.004122
12.295908	850.527816	12.009139
12.111524	841.642737	12.014157
11.958488	833.739802	12.019175
11.819329	852.332012	12.024192
12.024635	839.841051	12.029210
12.155191	843.654362	12.034227
11.693025	840.086574	12.039245
12.043372	833.001566	12.044263
12.231785	853.761384	12.049280
12.280834	868.485510	12.054298
11.995701	864.906764	12.059315
12.113696	872.760898	12.064333
12.628509	857.917317	12.069351
12.696691	871.400024	12.074368
12.596238	856.860449	12.079386
12.426146	837.484854	12.084403
11.885042	847.951674	12.089421
12.205293	844.049600	12.094439
12.087652	860.975084	12.099456
12.109895	855.719065	12.104474
12.486570	856.264338	12.109491
12.254759	867.891846	12.114509
12.498827	857.268733	12.119527
12.571873	863.063833	12.124544
12.553197	866.225261	12.129562
12.431662	860.345776	12.134579
12.330802	877.678175	12.139597
12.418682	859.401152	12.144615
12.404670	860.599466	12.149632
12.528050	857.106332	12.154650
12.603630	863.844544	12.159667
12.586614	871.507347	12.164685
13.144553	858.141312	12.169703
12.810306	864.549785	12.174720
12.403701	841.060775	12.179738
12.440930	845.947781	12.184755
12.596781	853.853217	12.189773
13.005599	860.874682	12.194791
12.350624	841.987604	12.199808
12.355217	831.899663	12.204826
12.650848	856.689551	12.209843
12.421142	859.705077	12.214861
12.452834	854.164970	12.219879
12.496317	866.479920	12.224896
12.540762	869.683663	12.229914
12.991912	866.784472	12.234931
12.575965	870.046783	12.239949
12.861454	866.351397	12.244967
12.513892	860.564669	12.249984
12.496890	871.395597	12.255002
12.907561	863.170396	12.260019
12.480980	861.495395	12.265037
12.886581	868.765874	12.270055
12.958238	863.589958	12.275072
12.408423	872.423588	12.280090
12.719643	862.432467	12.285107
12.344340	864.072407	12.290125
12.805284	862.598604	12.295143
13.116090	860.730398	12.300160
12.762445	861.289001	12.305178
12.709138	867.487297	12.310195
12.724504	872.968665	12.315213
12.791041	854.180603	12.320231
12.957608	859.404147	12.325248
12.533459	863.453890	12.330266
12.763820	858.927316	12.335283
12.583763	873.785945	12.340301
12.909003	879.868055	12.345319
13.113425	889.129411	12.350336
12.927157	895.218810	12.355354
13.255576	896.165984	12.360371
13.359097	891.826474	12.365389
13.158546	876.659344	12.370407
13.099853	879.854942	12.375424
12.776605	865.611777	12.380442
13.340337	859.255725	12.385459
13.153533	861.213564	12.390477
13.135215	861.280610	12.395495
13.364655	859.586254	12.400512
13.228227	872.763172	12.405530
13.323422	853.770607	12.410547
13.052415	858.127264	12.415565
13.521999	861.902560	12.420583
13.619705	867.330366	12.425600
13.296165	866.126634	12.430618
13.708133	858.172826	12.435635
13.392643	854.818252	12.440653
13.066109	835.665524	12.445671
13.097653	838.482684	12.450688
12.890444	858.281502	12.455706
13.498774	847.819220	12.460723
13.250051	855.727552	12.465741
13.077236	845.738495	12.470759
13.425142	858.620832	12.475776
13.006693	858.018801	12.480794
13.416899	858.952753	12.485811
13.271675	861.376667	12.490829
13.492387	856.641686	12.495847
13.206117	844.735706	12.500864
13.393191	854.928184	12.505882
13.611932	846.482394	12.510899
13.418046	845.614849	12.515917
12.859192	835.291734	12.520935
13.450167	839.803617	12.525952
13.246097	859.150621	12.530970
13.641613	845.026838	12.535987
13.363448	857.836293	12.541005
13.451090	865.755271	12.546023
12.972702	863.639405	12.551040
12.684730	864.039937	12.556058
13.305529	864.026948	12.561075
13.429462	868.467428	12.566093
13.395164	870.421617	12.571111
13.603589	865.167498	12.576128
13.219570	861.194145	12.581146
13.406342	863.870520	12.586163
13.408770	868.225095	12.591181
13.268394	864.580898	12.596199
13.715959	857.706445	12.601216
13.379566	857.637900	12.606234
13.308773	875.659789	12.611251
13.433815	894.206617	12.616269
13.478789	885.446080	12.621287
13.686859	899.387398	12.626304
13.270452	902.547645	12.631322
13.898010	895.325966	12.636339
13.572950	898.658091	12.641357
13.724131	905.506148	12.646375
13.759094	902.186250	12.651392
13.522637	886.406749	12.656410
13.851276	895.633312	12.661427
14.149219	891.409479	12.666445
13.978152	899.979388	12.671463
13.935796	885.918287	12.676480
14.110731	895.686300	12.681498
13.735405	866.740692	12.686515
13.609204	866.653156	12.691533
13.617262	861.680925	12.696551
13.762497	870.841343	12.701568
13.720244	894.735236	12.706586
13.839543	884.829252	12.711603
13.888444	895.473551	12.716621
13.883803	896.664611	12.721639
13.946385	889.451869	12.726656
13.460040	889.820039	12.731674
13.496363	878.380313	12.736691
13.955331	895.532632	12.741709
13.751754	889.733316	12.746727
13.964379	890.075526	12.751744
13.766929	897.956611	12.756762
13.385069	891.987973	12.761779
13.979804	894.473334	12.766797
13.897367	893.617875	12.771815
14.100180	892.722164	12.776832
13.974116	901.198825	12.781850
14.244083	896.626429	12.786867
14.164811	894.643581	12.791885
13.743151	890.451383	12.796903
14.162843	890.888089	12.801920
13.687897	891.686385	12.806938
14.363308	898.235146	12.811955
14.039041	895.100381	12.816973
14.133694	897.500896	12.821991
14.019467	894.739122	12.827008
14.575908	903.422031	12.832026
14.365204	891.676133	12.837043
13.898351	891.055038	12.842061
13.720821	895.544656	12.847079
14.262384	909.705330	12.852096
13.954601	916.837373	12.857114
13.966120	916.029760	12.862131
13.888380	933.732055	12.867149
14.182800	931.338590	12.872167
14.340894	925.641766	12.877184
14.049456	932.885071	12.882202
14.233155	920.605551	12.887219
14.636695	923.988600	12.892237
14.374193	916.731456	12.897255
14.848214	917.935328	12.902272
14.718516	922.828492	12.907290
14.390790	917.757923	12.912307
14.848848	925.766183	12.917325
14.700032	904.928091	12.922343
14.654543	885.725116	12.927360
14.385628	893.447173	12.932378
14.494642	879.031495	12.937395
14.687761	888.837042	12.942413
14.451744	887.856794	12.947431
14.468431	879.377854	12.952448
14.565012	893.527519	12.957466
14.444250	881.371265	12.962483
14.959335	881.434594	12.967501
14.466720	889.226584	12.972519
14.946790	884.456311	12.977536
14.489317	887.480945	12.982554
14.335699	873.121468	12.987571
14.458373	877.077698	12.992589
14.249863	883.217019	12.997607
14.370080	885.154925	13.002624
14.479921	878.417264	13.007642
14.274584	885.808002	13.012659
14.024132	895.856218	13.017677
14.216657	915.332106	13.022695
14.526025	912.296622	13.027712
14.677060	914.744406	13.032730
14.507993	918.210176	13.037747
14.860097	923.460550	13.042765
14.594028	930.219432	13.047783
14.660718	916.463158	13.052800
14.533538	927.586793	13.057818
14.476353	917.971718	13.062835
14.839267	917.688608	13.067853
14.669504	925.875804	13.072871
14.503639	920.025469	13.077888
14.749128	933.566217	13.082906
15.109300	938.712623	13.087923
14.992695	932.217837	13.092941
14.782252	923.584611	13.097959
14.700307	920.867390	13.102976
14.825394	956.730229	13.107994
14.903447	947.923153	13.113011
15.098005	951.243518	13.118029
15.080544	951.288084	13.123047
15.505020	943.204530	13.128064
14.663479	933.334785	13.133082
14.487879	936.174190	13.138099
15.243933	939.343798	13.143117
14.994792	946.764733	13.148135
14.976545	948.160865	13.153152
15.231894	953.141561	13.158170
14.957679	935.084692	13.163187
15.102056	936.297479	13.168205
15.047199	945.004087	13.173223
15.427227	929.953125	13.178240
14.965312	929.181731	13.183258
15.070220	922.901282	13.188275
15.136234	920.694259	13.193293
14.742328	924.360937	13.198311
15.244610	934.734309	13.203328
15.379590	951.301664	13.208346
15.119637	948.792663	13.213363
15.120886	949.511675	13.218381
15.506683	945.176476	13.223399
15.223427	941.136852	13.228416
15.110043	935.183367	13.233434
15.067584	948.226829	13.238451
15.331858	952.601431	13.243469
15.500283	946.402388	13.248487
15.322021	940.357278	13.253504
15.352336	955.084288	13.258522
15.163500	955.014188	13.263539
15.278621	949.205875	13.268557
15.034200	947.083806	13.273575
15.283591	946.580619	13.278592
15.551273	950.735897	13.283610
15.608951	938.673414	13.288627
15.440212	950.092859	13.293645
15.389212	945.140300	13.298663
15.594049	949.312163	13.303680
15.417808	952.484591	13.308698
15.263781	949.746114	13.313715
15.256497	934.052095	13.318733
15.225310	948.036146	13.323751
15.154426	948.334084	13.328768
15.397546	956.215409	13.333786
15.124610	947.703009	13.338803
15.428468	944.727277	13.343821
15.021655	955.032925	13.348839
15.244052	953.169871	13.353856
15.513769	960.779231	13.358874
15.380545	957.936545	13.363891
15.701675	964.512589	13.368909
15.439277	967.781036	13.373927
15.650112	969.403144	13.378944
16.000300	959.221595	13.383962
15.812855	967.408981	13.388979
15.950000	954.543333	13.393997
15.571250	966.978919	13.399015
15.741713	964.548464	13.404032
16.016459	967.091737	13.409050
15.763291	965.782781	13.414067
15.923270	958.985726	13.419085
16.153381	970.791556	13.424103
15.991115	966.502246	13.429120
15.939958	962.744283	13.434138
15.603921	963.884720	13.439155
15.658136	962.651322	13.444173
15.809214	954.828458	13.449191
15.997546	972.846410	13.454208
15.692903	969.158383	13.459226
15.898132	962.371660	13.464243
15.743309	960.678799	13.469261
15.801076	971.127132	13.474279
15.765788	970.753949	13.479296
16.070245	961.289479	13.484314
15.704889	967.145851	13.489331
15.930249	965.738033	13.494349
15.755744	971.859665	13.499367
15.913425	957.062314	13.504384
16.078779	955.995853	13.509402
16.139681	966.317997	13.514419
16.124054	962.467268	13.519437
15.656277	977.113256	13.524455
16.024999	970.743528	13.529472
16.065471	976.619829	13.534490
16.131146	995.338964	13.539507
16.374573	987.288161	13.544525
16.222102	995.427368	13.549543
16.174712	979.583264	13.554560
16.140954	972.744610	13.559578
16.034284	980.537814	13.564595
16.256065	986.308283	13.569613
16.499955	996.853018	13.574631
16.454959	978.656562	13.579648
16.224352	972.824877	13.584666
15.859380	972.834171	13.589683
16.248262	986.790464	13.594701
16.329438	986.647991	13.599719
16.575769	983.447744	13.604736
16.535690	982.199618	13.609754
16.277968	1003.258032	13.614771
16.174573	985.198855	13.619789
16.529906	983.967554	13.624807
16.324492	993.705096	13.629824
16.792591	984.274878	13.634842
16.507993	987.528004	13.639859
16.390212	990.151010	13.644877
16.696472	989.279037	13.649895
16.369434	994.483627	13.654912
16.422692	986.089022	13.659930
16.597908	988.896932	13.664947
16.702682	981.225776	13.669965
16.883445	992.853688	13.674983
16.305829	973.945396	13.680000
16.645546	968.307403	13.685018
16.511690	984.919813	13.690035
16.551707	987.658252	13.695053
16.455299	983.411292	13.700071
16.831850	980.650469	13.705088
16.958998	984.846301	13.710106
16.777436	983.959785	13.715123
16.818845	979.485067	13.720141
16.782069	964.620452	13.725159
16.759447	958.930354	13.730176
16.562348	946.500789	13.735194
16.439283	969.248316	13.740211
16.639568	970.911039	13.745229
16.900982	987.915039	13.750247
16.778257	987.661700	13.755264
16.851895	976.614779	13.760282
16.723896	979.886505	13.765299
16.701876	980.619107	13.770317
16.603805	979.529456	13.775335
16.627572	985.041656	13.780352
16.800859	981.205167	13.785370
16.787255	986.567762	13.790387
16.845300	992.927499	13.795405
16.881613	987.403310	13.800423
17.049384	989.691871	13.805440
17.288233	977.577669	13.810458
17.127947	986.392554	13.815475
17.121713	981.067786	13.820493
17.170242	988.131334	13.825511
17.114312	984.427590	13.830528
17.460715	980.144258	13.835546
17.120902	986.682419	13.840563
17.380418	990.457823	13.845581
16.957734	975.845917	13.850599
16.699197	989.367369	13.855616
17.082589	970.820648	13.860634
16.733774	987.808683	13.865651
17.111317	987.055223	13.870669
17.011458	974.800673	13.875687
16.706983	991.744580	13.880704
16.997853	977.514664	13.885722
16.978563	992.928039	13.890739
17.381051	1014.179574	13.895757
17.522033	1014.319490	13.900775
17.573150	1005.343339	13.905792
17.582125	988.455049	13.910810
16.902593	980.440065	13.915827
17.061719	992.796723	13.920845
17.635753	997.642007	13.925863
17.208849	1012.227247	13.930880
17.540352	1010.426949	13.935898
17.542385	1008.044397	13.940915
17.314080	1007.173477	13.945933
17.680338	1005.498712	13.950951
17.367382	999.251565	13.955968
17.723454	987.814123	13.960986
17.190201	993.539617	13.966003
17.373355	998.354435	13.971021
17.875827	1002.551227	13.976039
17.410354	995.519288	13.981056
17.267518	1003.411181	13.986074
17.321890	1009.116624	13.991091
17.591731	1016.862484	13.996109
17.702923	1014.617967	14.001127
17.174675	1015.949988	14.006144
17.384528	1009.974053	14.011162
17.655921	1018.875760	14.016179
17.525160	1017.402402	14.021197
17.475231	1015.610620	14.026215
17.518287	1022.992849	14.031232
17.645542	1009.487166	14.036250
17.308174	1012.958530	14.041267
17.621806	1013.517672	14.046285
17.862392	1012.325801	14.051303
17.411831	1032.774600	14.056320
17.938790	1035.909856	14.061338
17.978817	1042.459075	14.066355
18.074766	1030.140435	14.071373
18.064323	1016.202264	14.076391
18.004975	1010.660318	14.081408
17.784311	1009.694648	14.086426
18.074487	1011.826098	14.091443
17.849471	1017.454312	14.096461
17.989673	1003.946691	14.101479
17.881325	1014.121769	14.106496
18.051485	1012.472719	14.111514
17.939377	1013.674365	14.116531
17.908818	1012.353711	14.121549
18.305583	1010.544595	14.126567
17.723022	1010.763736	14.131584
17.996430	1029.370938	14.136602
18.119963	1034.741394	14.141619
17.757543	1047.464357	14.146637
18.108601	1041.869927	14.151655
18.035463	1042.551836	14.156672
18.140510	1043.238741	14.161690
18.269378	1049.614843	14.166707
18.215296	1042.633282	14.171725
18.325446	1043.882437	14.176743
18.180202	1049.360101	14.181760
18.505110	1046.711425	14.186778
18.374964	1043.507350	14.191795
18.375578	1043.274467	14.196813
18.243710	1034.867030	14.201831
17.845997	1029.778959	14.206848
18.349572	1033.102891	14.211866
18.531870	1034.912467	14.216883
18.051890	1044.755740	14.221901
18.267991	1031.069439	14.226919
18.345720	1047.632189	14.231936
18.777103	1041.215173	14.236954
18.323901	1045.407930	14.241971
18.542693	1049.493178	14.246989
18.512143	1045.447192	14.252007
18.449370	1053.388369	14.257024
18.750916	1041.802542	14.262042
18.526431	1049.334689	14.267059
18.512277	1052.979184	14.272077
18.794583	1047.742316	14.277095
18.486194	1039.356767	14.282112
18.454178	1052.203447	14.287130
18.587514	1051.173761	14.292147
18.422258	1053.006726	14.297165
18.451305	1040.471219	14.302183
18.620647	1047.718043	14.307200
18.853059	1045.995720	14.312218
18.653189	1049.243813	14.317235
18.576767	1049.955590	14.322253
18.720775	1045.194258	14.327271
18.649809	1052.790981	14.332288
18.402110	1049.248517	14.337306
18.672791	1039.936308	14.342323
18.763012	1038.529364	14.347341
18.793897	1035.490379	14.352359
18.871112	1036.885110	14.357376
18.643451	1036.790132	14.362394
18.745412	1031.150469	14.367411
18.494845	1042.798036	14.372429
18.811126	1042.854858	14.377447
18.549834	1043.165173	14.382464
18.935412	1061.337609	14.387482
18.955269	1053.319586	14.392499
18.986463	1060.654982	14.397517
18.984081	1060.018331	14.402535
18.934335	1063.688196	14.407552
19.052653	1066.755384	14.412570
19.288015	1062.159037	14.417587
18.962185	1064.729641	14.422605
19.321212	1071.304488	14.427623
19.105587	1063.497196	14.432640
19.558679	1070.597155	14.437658
19.040949	1050.880776	14.442675
18.792578	1049.154063	14.447693
19.298254	1047.066556	14.452711
19.140619	1060.953320	14.457728
19.259726	1063.301796	14.462746
19.162448	1065.793101	14.467763
19.345449	1064.304888	14.472781
19.371686	1067.669530	14.477799
19.067389	1060.736789	14.482816
19.196610	1061.795031	14.487834
19.306729	1058.626037	14.492851
19.185337	1063.527812	14.497869
19.202219	1054.752927	14.502887
19.092575	1061.788228	14.507904
19.036094	1066.094139	14.512922
19.192879	1058.719515	14.517939
18.980531	1068.911619	14.522957
19.520090	1056.470246	14.527975
19.390003	1063.860836	14.532992
18.953506	1069.692690	14.538010
19.159999	1067.055511	14.543027
19.356904	1088.196659	14.548045
19.523666	1085.957119	14.553063
19.510786	1085.121054	14.558080
19.551957	1096.954663	14.563098
19.838684	1089.167079	14.568115
19.490934	1089.385204	14.573133
19.487679	1080.183585	14.578151
19.702040	1082.052621	14.583168
19.645368	1088.244476	14.588186
19.803938	1080.397775	14.593203
19.595975	1089.526353	14.598221
19.990464	1078.891514	14.603239
19.629042	1089.299378	14.608256
19.679849	1093.551155	14.613274
20.033928	1088.967460	14.618291
20.031187	1093.499695	14.623309
20.144403	1094.249415	14.628327
20.377503	1080.167019	14.633344
19.749057	1064.580243	14.638362
19.798433	1062.866517	14.643379
19.668443	1066.759844	14.648397
19.807126	1077.562532	14.653415
20.053907	1087.243217	14.658432
19.561927	1089.587387	14.663450
20.033291	1078.731414	14.668467
20.087562	1086.824891	14.673485
19.943250	1083.554065	14.678503
20.272739	1080.347043	14.683520
19.969771	1087.982123	14.688538
20.101233	1088.995712	14.693555
20.183955	1086.512623	14.698573
20.141181	1082.650310	14.703591
19.834547	1085.953646	14.708608
20.042144	1082.762436	14.713626
20.079687	1072.665054	14.718643
19.957567	1088.395271	14.723661
20.080178	1087.191007	14.728679
20.318198	1081.280063	14.733696
19.734939	1085.895439	14.738714
19.959992	1080.495806	14.743731
20.072472	1092.409147	14.748749
19.956595	1087.676186	14.753767
20.062408	1105.385740	14.758784
20.132616	1114.048156	14.763802
20.417468	1105.915065	14.768819
20.435704	1124.112854	14.773837
20.243186	1112.231127	14.778855
20.347867	1119.376090	14.783872
20.195514	1116.805487	14.788890
20.524115	1120.366588	14.793907
20.327425	1119.590420	14.798925
20.666135	1119.317211	14.803943
20.777568	1115.275691	14.808960
20.625661	1112.826845	14.813978
20.743613	1102.255798	14.818995
20.306419	1120.779987	14.824013
20.375517	1111.033212	14.829031
20.470366	1122.070697	14.834048
20.646740	1112.126695	14.839066
20.652419	1120.167009	14.844083
20.609038	1121.050859	14.849101
20.811150	1114.052316	14.854119
20.908748	1122.200452	14.859136
20.386537	1114.848852	14.864154
20.581876	1120.981951	14.869171
20.745447	1115.925483	14.874189
20.519977	1121.278264	14.879207
20.761915	1110.231087	14.884224
20.568936	1109.572004	14.889242
20.415488	1115.996757	14.894259
20.922481	1127.228888	14.899277
20.869877	1119.760512	14.904295
20.847231	1137.865878	14.909312
20.839585	1134.839341	14.914330
20.920360	1148.384471	14.919347
21.067606	1148.926241	14.924365
21.032204	1143.301366	14.929383
20.883558	1145.320936	14.934400
20.941507	1148.159178	14.939418
21.195542	1150.837282	14.944435
21.348328	1144.261180	14.949453
21.293866	1139.607212	14.954471
21.028911	1113.567521	14.959488
20.886845	1122.041831	14.964506
21.185770	1120.175853	14.969523
21.185834	1133.215102	14.974541
21.227845	1145.372178	14.979559
21.069625	1142.760224	14.984576
20.966018	1146.386853	14.989594
21.243284	1143.209704	14.994611
21.497418	1142.708779	14.999629
21.245061	1156.744725	15.004647
21.248330	1138.615485	15.009664
21.231646	1147.050193	15.014682
21.288569	1138.844927	15.019699
21.641246	1145.958760	15.024717
21.433121	1157.562988	15.029735
21.261653	1136.590454	15.034752
21.308937	1142.512240	15.039770
21.539548	1145.437481	15.044787
21.272727	1144.709313	15.049805
21.456390	1140.627901	15.054823
21.596518	1139.355788	15.059840
21.541227	1151.426603	15.064858
21.782703	1153.520460	15.069875
21.319008	1143.461188	15.074893
21.235029	1138.718216	15.079911
21.384225	1142.045824	15.084928
21.538599	1152.679463	15.089946
21.681405	1152.931856	15.094963
21.893812	1153.299892	15.099981
21.197625	1150.878596	15.104999
21.521754	1140.326787	15.110016
21.443667	1142.126069	15.115034
21.566371	1157.526377	15.120051
21.393562	1162.824808	15.125069
21.192026	1182.785282	15.130087
21.622923	1164.836090	15.135104
21.485793	1173.963443	15.140122
21.639251	1171.791040	15.145139
21.547079	1169.255948	15.150157
21.645001	1175.798608	15.155175
22.022423	1189.276250	15.160192
21.867998	1197.976230	15.165210
22.210292	1208.544016	15.170227
22.091881	1204.937637	15.175245
21.940499	1199.937520	15.180263
22.224922	1192.138850	15.185280
22.078997	1186.046474	15.190298
21.839176	1181.565426	15.195315
22.394945	1182.850382	15.200333
22.212015	1176.691302	15.205351
22.283291	1169.544501	15.210368
21.971804	1175.252406	15.215386
22.156180	1175.035208	15.220403
22.072598	1164.745809	15.225421
21.956374	1183.343387	15.230439
22.232993	1190.875848	15.235456
22.524613	1207.895274	15.240474
22.468083	1198.241437	15.245491
22.094262	1183.252910	15.250509
22.117922	1202.323575	15.255527
22.341063	1197.753024	15.260544
22.212695	1200.301645	15.265562
22.145069	1202.516068	15.270579
22.376036	1205.542624	15.275597
22.219030	1216.080348	15.280615
22.173635	1199.284066	15.285632
22.095130	1207.296809	15.290650
22.330336	1192.896887	15.295667
22.256685	1194.032555	15.300685
22.362334	1206.411015	15.305703
22.452612	1203.484996	15.310720
22.635318	1225.253384	15.315738
22.676316	1226.985955	15.320755
22.673304	1219.648290	15.325773
22.498413	1211.515541	15.330791
22.439838	1228.880613	15.335808
22.549405	1235.003132	15.340826
22.731396	1243.183638	15.345843
22.692829	1231.988666	15.350861
22.935708	1240.729098	15.355879
23.112264	1231.310301	15.360896
23.197715	1234.582726	15.365914
22.648172	1218.558410	15.370931
23.042598	1207.870746	15.375949
22.990621	1215.397689	15.380967
22.815306	1203.760646	15.385984
22.660215	1199.594869	15.391002
23.150846	1224.943485	15.396019
23.066580	1226.533397	15.401037
23.047357	1208.993526	15.406055
23.203149	1203.606478	15.411072
22.898260	1206.969581	15.416090
22.860911	1203.337210	15.421107
23.165994	1209.528377	15.426125
22.901386	1220.593451	15.431143
23.059215	1232.850138	15.436160
23.015060	1221.349650	15.441178
23.120180	1234.051201	15.446195
22.988794	1226.661924	15.451213
22.740734	1233.704432	15.456231
22.949340	1238.876481	15.461248
22.897242	1236.381204	15.466266
23.224351	1239.818780	15.471283
23.288991	1229.332429	15.476301
23.023785	1231.096512	15.481319
22.705367	1234.704535	15.486336
23.018575	1246.764717	15.491354
22.950504	1258.903269	15.496371
23.263446	1265.306119	15.501389
23.179577	1270.762106	15.506407
23.515870	1268.259127	15.511424
23.506445	1263.940342	15.516442
23.073228	1262.075477	15.521459
23.397810	1254.989318	15.526477
23.216787	1266.512390	15.531495
23.353511	1262.267469	15.536512
23.468213	1272.091732	15.541530
23.872011	1278.305584	15.546547
23.699091	1276.432144	15.551565
23.834412	1273.515988	15.556583
23.606693	1267.440050	15.561600
23.555619	1262.117281	15.566618
23.625188	1265.371867	15.571635
23.794887	1260.124212	15.576653
23.781788	1268.389128	15.581671
23.640105	1273.091796	15.586688
23.928889	1279.898583	15.591706
23.715477	1287.548878	15.596723
24.221982	1280.717049	15.601741
24.145791	1282.032643	15.606759
23.943092	1264.201032	15.611776
23.849265	1264.170339	15.616794
23.583461	1259.025751	15.621811
23.871809	1272.872463	15.626829
24.094000	1280.268906	15.631847
24.102242	1280.440208	15.636864
24.154105	1290.907054	15.641882
24.064202	1283.017860	15.646899
24.316014	1269.934408	15.651917
23.781953	1266.967088	15.656935
23.917680	1285.921320	15.661952
24.249659	1289.159708	15.666970
24.053005	1286.726495	15.671987
24.401505	1291.087768	15.677005
24.566460	1301.002352	15.682023
24.422760	1284.200573	15.687040
24.180269	1276.902850	15.692058
24.006264	1268.062160	15.697075
24.633911	1274.157927	15.702093
24.347068	1285.578046	15.707111
24.391956	1284.606459	15.712128
24.418418	1273.278092	15.717146
24.400820	1279.588154	15.722163
24.250917	1287.335221	15.727181
24.511460	1288.930746	15.732199
24.383310	1286.682639	15.737216
24.649816	1287.857361	15.742234
24.492254	1288.229069	15.747251
24.482546	1279.077013	15.752269
24.274140	1290.943158	15.757287
24.424152	1285.542078	15.762304
24.335679	1274.847767	15.767322
24.123886	1282.276960	15.772339
24.642838	1294.543889	15.777357
24.618319	1283.271964	15.782375
24.427747	1280.236461	15.787392
24.459653	1291.597217	15.792410
24.434736	1298.312766	15.797427
24.844200	1310.935152	15.802445
24.790466	1322.877911	15.807463
24.652472	1320.713894	15.812480
25.046205	1318.896979	15.817498
24.754675	1327.689954	15.822515
25.026762	1318.175211	15.827533
24.792401	1323.276813	15.832551
24.779365	1320.122607	15.837568
25.342027	1309.065193	15.842586
24.863165	1310.966744	15.847603
25.018134	1323.096436	15.852621
24.852847	1315.079350	15.857639
24.915345	1325.061661	15.862656
24.903312	1316.082578	15.867674
24.651700	1323.878947	15.872691
25.037629	1312.357308	15.877709
24.761186	1318.384424	15.882727
25.009381	1326.570567	15.887744
25.170740	1330.294177	15.892762
25.270711	1342.984663	15.897779
25.151961	1340.207515	15.902797
25.190159	1343.950892	15.907815
24.935775	1354.351479	15.912832
25.163773	1344.977450	15.917850
25.069804	1358.078288	15.922867
25.166426	1349.688423	15.927885
25.585823	1344.073932	15.932903
25.518221	1354.384212	15.937920
25.633012	1346.373770	15.942938
24.823097	1349.751672	15.947955
25.152554	1347.882984	15.952973
25.448583	1348.660961	15.957991
25.313762	1347.269529	15.963008
25.652888	1344.946161	15.968026
25.494637	1340.301608	15.973043
25.746227	1358.973633	15.978061
25.734878	1360.599927	15.983079
25.860747	1366.266132	15.988096
25.656738	1358.389655	15.993114
25.284083	1353.106811	15.998131
25.694285	1375.299951	16.003149
25.740714	1375.501553	16.008167
25.917697	1371.500503	16.013184
26.242246	1382.332917	16.018202
25.600533	1368.157659	16.023219
25.895651	1380.682875	16.028237
25.995716	1375.529943	16.033255
26.166526	1373.066694	16.038272
26.296786	1370.964229	16.043290
26.109942	1364.031820	16.048307
25.761525	1347.061275	16.053325
26.285817	1350.606033	16.058343
26.164790	1361.644134	16.063360
26.192930	1345.222098	16.068378
25.859544	1349.174893	16.073395
26.026280	1344.431757	16.078413
25.842805	1363.174110	16.083431
26.037715	1368.530526	16.088448
26.275866	1370.089608	16.093466
26.303046	1380.159472	16.098483
26.135217	1375.833965	16.103501
26.236225	1374.673990	16.108519
26.158814	1372.254714	16.113536
26.406354	1369.156831	16.118554
26.343315	1368.885060	16.123571
26.289743	1367.664621	16.128589
26.300546	1364.114398	16.133607
26.003795	1378.263378	16.138624
26.351167	1377.161691	16.143642
26.299196	1375.111384	16.148659
26.385618	1364.793560	16.153677
26.733893	1365.833533	16.158695
26.265487	1383.783950	16.163712
26.495319	1379.607850	16.168730
26.381228	1380.136722	16.173747
26.225582	1390.841048	16.178765
26.727992	1393.574001	16.183783
26.703934	1400.263078	16.188800
26.555802	1398.466420	16.193818
26.455832	1397.852968	16.198835
26.617271	1394.759467	16.203853
26.825910	1397.017423	16.208871
26.359278	1405.581543	16.213888
26.627327	1406.335017	16.218906
26.523848	1401.470795	16.223923
26.544008	1405.273065	16.228941
26.692755	1419.814535	16.233959
26.919137	1430.913367	16.238976
26.952970	1436.166326	16.243994
26.872850	1436.097545	16.249011
26.645596	1435.052041	16.254029
27.048573	1435.501567	16.259047
26.975502	1449.312706	16.264064
27.187956	1434.788778	16.269082
27.133024	1423.507211	16.274099
26.735624	1438.967968	16.279117
27.088149	1430.220066	16.284135
27.045212	1428.993928	16.289152
27.204324	1421.451448	16.294170
27.123960	1433.713805	16.299187
27.149793	1439.126135	16.304205
27.122791	1427.152647	16.309223
27.084300	1443.907445	16.314240
27.726127	1443.526865	16.319258
27.677587	1454.616036	16.324275
27.616434	1435.696420	16.329293
27.356791	1421.047795	16.334311
27.424487	1414.225441	16.339328
27.600988	1422.440607	16.344346
27.711714	1419.156888	16.349363
27.465943	1423.359358	16.354381
27.843620	1415.099757	16.359399
27.539901	1424.013091	16.364416
27.672854	1422.776584	16.369434
27.590082	1418.751529	16.374451
27.349737	1422.388223	16.379469
27.631933	1428.821416	16.384487
27.835743	1448.285388	16.389504
27.902739	1439.813964	16.394522
27.936389	1449.808799	16.399539
28.050871	1439.559506	16.404557
27.876242	1427.033725	16.409575
27.574592	1434.088526	16.414592
28.056948	1431.329527	16.419610
28.047643	1443.573654	16.424627
27.765916	1449.945346	16.429645
28.343599	1454.736836	16.434663
27.780012	1455.181354	16.439680
28.080226	1456.322570	16.444698
27.994896	1459.044214	16.449715
27.983541	1459.084918	16.454733
28.215873	1453.994145	16.459751
28.104306	1455.801161	16.464768
28.279035	1457.611644	16.469786
28.199196	1453.606368	16.474803
28.106896	1460.988345	16.479821
28.350600	1452.701658	16.484839
28.125928	1460.020679	16.489856
28.366199	1448.484039	16.494874
28.200500	1454.641508	16.499891
27.813190	1453.374654	16.504909
28.298288	1446.939935	16.509927
28.104985	1458.880868	16.514944
28.086583	1458.754256	16.519962
28.342652	1454.539160	16.524979
27.963695	1473.309031	16.529997
28.412224	1482.412607	16.535015
28.374962	1480.720041	16.540032
28.564277	1486.106158	16.545050
28.695233	1485.981828	16.550067
28.370286	1496.117045	16.555085
28.700542	1480.130304	16.560103
28.485805	1485.791629	16.565120
28.694204	1483.793148	16.570138
28.742975	1484.115804	16.575155
28.703330	1497.675631	16.580173
28.907304	1480.852004	16.585191
28.958195	1497.897165	16.590208
28.693693	1481.836293	16.595226
29.019630	1491.053821	16.600243
28.984202	1492.801612	16.605261
29.157967	1488.258620	16.610279
28.959726	1483.118340	16.615296
28.878123	1482.106630	16.620314
29.022950	1480.901025	16.625331
29.055720	1482.820589	16.630349
29.116061	1478.532138	16.635367
28.898996	1488.357240	16.640384
28.826878	1470.581753	16.645402
29.217509	1477.146631	16.650419
28.742929	1477.967724	16.655437
29.133654	1485.985537	16.660455
29.376686	1504.873493	16.665472
29.070540	1501.673017	16.670490
29.537566	1508.112898	16.675507
29.407293	1514.657789	16.680525
29.691150	1507.096029	16.685543
29.271193	1505.530277	16.690560
29.148163	1485.153707	16.695578
29.605448	1494.869536	16.700595
29.492217	1508.605881	16.705613
29.553309	1504.614501	16.710631
29.517821	1504.699148	16.715648
29.439434	1509.179449	16.720666
29.312466	1506.729961	16.725683
29.159493	1515.452711	16.730701
29.504006	1503.382733	16.735719
29.562238	1508.350228	16.740736
29.487720	1506.330397	16.745754
29.573122	1506.969987	16.750771
29.318774	1516.190329	16.755789
29.572856	1513.713100	16.760807
29.612254	1532.542629	16.765824
29.688443	1538.689484	16.770842
30.117152	1537.641068	16.775859
30.016447	1545.794250	16.780877
29.870205	1533.952574	16.785895
29.898730	1534.969033	16.790912
30.120371	1536.192719	16.795930
30.295713	1530.857043	16.800947
30.087373	1536.551970	16.805965
30.289388	1538.009183	16.810983
30.029935	1533.750930	16.816000
30.201704	1542.919370	16.821018
30.233948	1532.878264	16.826035
30.279360	1545.149448	16.831053
30.546410	1530.042273	16.836071
30.396635	1529.613203	16.841088
30.007727	1534.746516	16.846106
30.395247	1525.615664	16.851123
30.453126	1541.643520	16.856141
30.402193	1533.870771	16.861159
30.188322	1532.635870	16.866176
30.096944	1538.617924	16.871194
30.268790	1530.445615	16.876211
30.047424	1540.884566	16.881229
30.056614	1532.921789	16.886247
30.475799	1531.153393	16.891264
30.010182	1535.612666	16.896282
30.520077	1541.534720	16.901299
30.659847	1560.272116	16.906317
30.754572	1556.356453	16.911335
30.629938	1560.096677	16.916352
30.807994	1556.391820	16.921370
30.995845	1556.663544	16.926387
30.729788	1561.453182	16.931405
30.953003	1555.032370	16.936423
30.951723	1554.799005	16.941440
30.907074	1562.382969	16.946458
30.831016	1556.954793	16.951475
31.076067	1554.448740	16.956493
30.995846	1560.270514	16.961511
31.221706	1558.454153	16.966528
31.278369	1538.208424	16.971546
31.176978	1527.145847	16.976563
30.879640	1531.964264	16.981581
30.981852	1516.545414	16.986599
31.013025	1527.266002	16.991616
30.808432	1548.173781	16.996634
31.383210	1543.187192	17.001651
31.193590	1553.209740	17.006669
31.359614	1555.295653	17.011687
31.628890	1558.189390	17.016704
31.371620	1556.680595	17.021722
31.749519	1548.895034	17.026739
31.261561	1556.419990	17.031757
31.008696	1548.238342	17.036775
31.559098	1544.940591	17.041792
31.522049	1549.462294	17.046810
31.465246	1545.001871	17.051827
31.639904	1558.407061	17.056845
31.288786	1552.050261	17.061863
31.587416	1553.048853	17.066880
31.403250	1553.214165	17.071898
31.845711	1546.805543	17.076915
31.346084	1550.639031	17.081933
31.449690	1545.865720	17.086951
31.593357	1551.204687	17.091968
31.544241	1552.162138	17.096986
31.768531	1551.289215	17.102003
31.587983	1562.716969	17.107021
31.822107	1573.259975	17.112039
31.819546	1584.376283	17.117056
31.686687	1583.512978	17.122074
31.891180	1586.002915	17.127091
31.848365	1579.006651	17.132109
31.953989	1579.630305	17.137127
32.078794	1577.026812	17.142144
31.823366	1579.425650	17.147162
32.008529	1578.509790	17.152179
31.953025	1584.041307	17.157197
31.707525	1591.493145	17.162215
31.780010	1588.740050	17.167232
32.046588	1607.204219	17.172250
32.241209	1606.950288	17.177267
32.466409	1605.178119	17.182285
32.462150	1606.906994	17.187303
32.286304	1603.554665	17.192320
32.535992	1610.770960	17.197338
32.948320	1613.978622	17.202355
32.778705	1604.214496	17.207373
32.665605	1612.167033	17.212391
32.715790	1606.999238	17.217408
32.798320	1605.135898	17.222426
32.530514	1587.055060	17.227443
32.621793	1587.403760	17.232461
32.698131	1594.922477	17.237479
32.788620	1587.696530	17.242496
32.679486	1587.407966	17.247514
32.989564	1604.397817	17.252531
32.771762	1593.483350	17.257549
32.590986	1582.130349	17.262567
32.898410	1582.248473	17.267584
32.793278	1598.383238	17.272602
32.937000	1597.899168	17.277619
33.117771	1597.100159	17.282637
32.924512	1607.371146	17.287655
33.280137	1596.338098	17.292672
33.080554	1610.289564	17.297690
33.172342	1595.194952	17.302707
33.054778	1592.049895	17.307725
32.838897	1597.841157	17.312743
33.019677	1594.795988	17.317760
32.972448	1606.927237	17.322778
33.140298	1595.084191	17.327795
33.252846	1597.657229	17.332813
32.892171	1600.673384	17.337831
33.282251	1583.526014	17.342848
33.019110	1599.043868	17.347866
33.361093	1587.948916	17.352883
33.090010	1593.968758	17.357901
33.263932	1612.001257	17.362919
33.387678	1618.818542	17.367936
33.576376	1623.711961	17.372954
33.585276	1629.585561	17.377971
33.634931	1627.454261	17.382989
33.487319	1626.773682	17.388007
33.510202	1629.481213	17.393024
33.152529	1629.701377	17.398042
33.339704	1627.174368	17.403059
33.467561	1627.285362	17.408077
33.450035	1623.756688	17.413095
33.822684	1647.535551	17.418112
33.761757	1653.787778	17.423130
34.418222	1652.636567	17.428147
34.047111	1648.653000	17.433165
33.589893	1635.428374	17.438183
34.013364	1630.210102	17.443200
33.874841	1649.089844	17.448218
34.270119	1654.055026	17.453235
34.105426	1650.068445	17.458253
34.279955	1657.930958	17.463271
34.698745	1648.643114	17.468288
34.452807	1644.950437	17.473306
34.103861	1621.897395	17.478323
34.416397	1615.549974	17.483341
34.223013	1622.181511	17.488359
34.419653	1622.698012	17.493376
34.250635	1623.829395	17.498394
34.268674	1642.488399	17.503411
34.500429	1636.530255	17.508429
34.364412	1646.668793	17.513447
34.622741	1641.914366	17.518464
34.639490	1649.770080	17.523482
34.667703	1646.316115	17.528499
34.695737	1643.292636	17.533517
34.570492	1653.218402	17.538535
34.517168	1638.859250	17.543552
34.551387	1644.327149	17.548570
34.513610	1643.572127	17.553587
34.772716	1637.800579	17.558605
34.395738	1644.619728	17.563623
34.646119	1648.398184	17.568640
34.697083	1646.836474	17.573658
34.732353	1640.027252	17.578675
35.073837	1645.001911	17.583693
34.600876	1652.436651	17.588711
34.691230	1644.780244	17.593728
35.004502	1653.427399	17.598746
34.949954	1675.052781	17.603763
35.232093	1667.874446	17.608781
35.008694	1683.776514	17.613799
35.137517	1664.883087	17.618816
35.258704	1676.377385	17.623834
35.184486	1671.187614	17.628851
35.315400	1673.048468	17.633869
35.253284	1684.449261	17.638887
35.838725	1670.984393	17.643904
35.360024	1666.698563	17.648922
35.618289	1670.335386	17.653939
35.527493	1677.983718	17.658957
35.445273	1673.116881	17.663975
35.337034	1675.136730	17.668992
35.290564	1673.678509	17.674010
35.486728	1675.077851	17.679027
35.680930	1666.213086	17.684045
35.485349	1674.096422	17.689063
35.526594	1670.833974	17.694080
35.509544	1672.963147	17.699098
35.234166	1675.280071	17.704115
35.442645	1669.663316	17.709133
35.301756	1679.207874	17.714151
35.585369	1693.561392	17.719168
35.892654	1687.677350	17.724186
35.808534	1698.607834	17.729203
35.935480	1693.243884	17.734221
35.842000	1692.837195	17.739239
35.951607	1688.386036	17.744256
35.725298	1699.605536	17.749274
35.864017	1690.916637	17.754291
35.786880	1688.235882	17.759309
35.975916	1708.410999	17.764327
36.459153	1716.471708	17.769344
36.455965	1717.375915	17.774362
36.452847	1717.694357	17.779379
36.579734	1702.371231	17.784397
36.570790	1692.378947	17.789415
36.486151	1693.089946	17.794432
36.207225	1688.498297	17.799450
36.045202	1700.240570	17.804467
36.682907	1713.171196	17.809485
36.682645	1714.585289	17.814503
36.860713	1717.728155	17.819520
36.896739	1697.334269	17.824538
36.349745	1697.158018	17.829555
37.077626	1697.381835	17.834573
37.039912	1698.284661	17.839591
36.709570	1687.386166	17.844608
36.595843	1690.703808	17.849626
36.916066	1685.155577	17.854643
36.889649	1686.645043	17.859661
36.713431	1699.000608	17.864679
36.618360	1705.310263	17.869696
36.966026	1715.916286	17.874714
37.127686	1723.347157	17.879731
37.228196	1724.546393	17.884749
37.133346	1734.347911	17.889767
36.755387	1720.477317	17.894784
37.018229	1727.391137	17.899802
36.872059	1719.417328	17.904819
37.183301	1723.649467	17.909837
36.964170	1726.384806	17.914855
36.862921	1726.425407	17.919872
36.898846	1717.825518	17.924890
37.100379	1723.373459	17.929907
37.555657	1738.873701	17.934925
37.748705	1750.421722	17.939943
37.459828	1730.283231	17.944960
37.454106	1724.818965	17.949978
37.094026	1728.035414	17.954995
37.580607	1741.721459	17.960013
37.399837	1741.834053	17.965031
37.754349	1746.534776	17.970048
37.675900	1741.694849	17.975066
37.815042	1745.284848	17.980083
37.799907	1740.686199	17.985101
37.759306	1740.380008	17.990119
37.712844	1732.688497	17.995136
38.109651	1732.636556	18.000154
37.727793	1739.503792	18.005171
38.088811	1738.654715	18.010189
37.902131	1738.471669	18.015207
38.150948	1734.738541	18.020224
38.237136	1728.930780	18.025242
37.926192	1736.802704	18.030259
38.392534	1720.073236	18.035277
38.059206	1723.902706	18.040295
37.930522	1731.378412	18.045312
38.234532	1733.335260	18.050330
38.413661	1737.424491	18.055347
38.583487	1729.612997	18.060365
38.041842	1733.764458	18.065383
38.183005	1736.366251	18.070400
38.439394	1730.253428	18.075418
38.388352	1736.836297	18.080435
38.223130	1724.714180	18.085453
38.275087	1735.524577	18.090471
38.471462	1756.067200	18.095488
38.824113	1757.371800	18.100506
38.605595	1768.902426	18.105523
38.938520	1770.431324	18.110541
38.951646	1768.784920	18.115559
39.071290	1767.789336	18.120576
38.888825	1758.027433	18.125594
39.010102	1745.785521	18.130611
38.958488	1737.444939	18.135629
38.599256	1734.428952	18.140647
39.168862	1752.946946	18.145664
39.306800	1754.216171	18.150682
38.866859	1739.993642	18.155699
38.891543	1745.555267	18.160717
39.233591	1763.246223	18.165735
39.019024	1755.073487	18.170752
39.120638	1760.184270	18.175770
39.124623	1765.050392	18.180787
39.313625	1762.795861	18.185805
39.308521	1769.312695	18.190823
39.225771	1775.931919	18.195840
39.121720	1766.658566	18.200858
38.967980	1766.164207	18.205875
39.145189	1771.410711	18.210893
38.914106	1770.239847	18.215911
39.298499	1772.894550	18.220928
39.639703	1789.153171	18.225946
39.318377	1787.872235	18.230963
39.521919	1782.247004	18.235981
39.517780	1786.982799	18.240999
39.363713	1793.523670	18.246016
39.816332	1776.379333	18.251034
39.648028	1780.567325	18.256051
39.526939	1780.999544	18.261069
39.609164	1785.503573	18.266087
39.840479	1801.913816	18.271104
40.135768	1806.082677	18.276122
39.884326	1813.908788	18.281139
40.605431	1803.687926	18.286157
40.197835	1797.070705	18.291175
39.914269	1783.392894	18.296192
40.070778	1778.536172	18.301210
40.255485	1796.664141	18.306227
40.522149	1795.083500	18.311245
40.446062	1785.066036	18.316263
39.956774	1779.259077	18.321280
40.091554	1772.714026	18.326298
40.255218	1799.919770	18.331315
40.389031	1794.203511	18.336333
40.328381	1802.902703	18.341351
40.305399	1812.584139	18.346368
40.252067	1805.571205	18.351386
40.080520	1809.886695	18.356403
40.398592	1804.098649	18.361421
40.358613	1811.622719	18.366439
40.560321	1819.305254	18.371456
40.988528	1838.993041	18.376474
40.986111	1842.554887	18.381491
40.962018	1838.928245	18.386509
41.036540	1841.069667	18.391527
40.889350	1833.998224	18.396544
41.180040	1820.736838	18.401562
41.022061	1829.533222	18.406579
41.052539	1826.477614	18.411597
41.486740	1826.560029	18.416615
41.055464	1805.258301	18.421632
41.131413	1802.526837	18.426650
40.886554	1801.969394	18.431667
41.075730	1819.548489	18.436685
41.582530	1822.712634	18.441703
41.354595	1836.066698	18.446720
41.375382	1825.365168	18.451738
41.296936	1830.565368	18.456755
41.343183	1819.086299	18.461773
41.508766	1828.553929	18.466791
41.249194	1828.597862	18.471808
41.617075	1826.771188	18.476826
41.460445	1836.554637	18.481843
41.211806	1822.267351	18.486861
41.392744	1819.313440	18.491879
41.095618	1840.054447	18.496896
41.499644	1840.240656	18.501914
41.044313	1859.694405	18.506931
41.694452	1855.887842	18.511949
41.674331	1859.958071	18.516967
41.616127	1862.239724	18.521984
41.968948	1853.247666	18.527002
41.547898	1870.041150	18.532019
42.041055	1871.229836	18.537037
42.427023	1876.771760	18.542055
42.666238	1889.191486	18.547072
42.571721	1868.978966	18.552090
42.588520	1865.596516	18.557107
42.351694	1861.796977	18.562125
42.583056	1851.027168	18.567143
42.378259	1852.607933	18.572160
42.542004	1848.432787	18.577178
42.464589	1850.794376	18.582195
42.426328	1847.261598	18.587213
42.727872	1841.640423	18.592231
42.402913	1846.972694	18.597248
42.401852	1847.682289	18.602266
42.326585	1840.250376	18.607283
42.237654	1853.201607	18.612301
42.554111	1854.809800	18.617319
42.457368	1870.826351	18.622336
42.659718	1867.650020	18.627354
42.831548	1874.511829	18.632371
42.764060	1881.129757	18.637389
42.789634	1874.658806	18.642407
42.768885	1875.693666	18.647424
42.944056	1869.359788	18.652442
42.863664	1881.174920	18.657459
42.788633	1881.677868	18.662477
42.709077	1883.135981	18.667495
42.637702	1887.669754	18.672512
43.272130	1903.210824	18.677530
43.168530	1907.445632	18.682547
43.295635	1908.387957	18.687565
43.447912	1901.174485	18.692583
43.522750	1907.623842	18.697600
43.412611	1905.975552	18.702618
43.421521	1907.527895	18.707635
43.196320	1904.773156	18.712653
43.458312	1905.173564	18.717671
43.462987	1908.677371	18.722688
43.881224	1898.505120	18.727706
43.695663	1900.763144	18.732723
43.350408	1904.306276	18.737741
43.686285	1894.358244	18.742759
43.352818	1906.994066	18.747776
43.538313	1918.352735	18.752794
43.640276	1922.938376	18.757811
43.663240	1926.482860	18.762829
43.960521	1923.337872	18.767847
43.797614	1939.279807	18.772864
44.201959	1931.975851	18.777882
44.023844	1932.200790	18.782899
43.967552	1928.554647	18.787917
44.238518	1922.856026	18.792935
44.422870	1923.187975	18.797952
44.340746	1928.695277	18.802970
44.368642	1927.797907	18.807987
44.375596	1928.167045	18.813005
44.534106	1926.663706	18.818023
44.358672	1931.598897	18.823040
44.684932	1923.305402	18.828058
44.723755	1920.683781	18.833075
44.336787	1933.197378	18.838093
44.548095	1922.832955	18.843111
44.766630	1946.016361	18.848128
44.768304	1940.189813	18.853146
44.590296	1937.541824	18.858163
44.778084	1949.894516	18.863181
44.925151	1949.141999	18.868199
44.766101	1958.919431	18.873216
44.836185	1951.677790	18.878234
44.957717	1956.918796	18.883251
45.314640	1964.051008	18.888269
45.257728	1940.767948	18.893287
45.036924	1950.168614	18.898304
45.040811	1939.395002	18.903322
45.165003	1947.145327	18.908339
45.271806	1952.852297	18.913357
45.484049	1942.346579	18.918375
45.306382	1951.303158	18.923392
45.109942	1941.971156	18.928410
45.351267	1944.023027	18.933427
45.222378	1944.147321	18.938445
45.641818	1943.163791	18.943463
45.570004	1945.171357	18.948480
45.460825	1945.734865	18.953498
45.534746	1949.427412	18.958515
45.378437	1942.769585	18.963533
45.758469	1948.703812	18.968551
45.487342	1966.085943	18.973568
45.828487	1972.724364	18.978586
45.477605	1973.940348	18.983603
45.491891	1981.063449	18.988621
45.627759	1966.817594	18.993639
45.575127	1972.297206	18.998656
45.988872	1962.560451	19.003674
46.223783	1968.749942	19.008691
46.196207	1973.110378	19.013709
46.332704	1969.074924	19.018727
46.120622	1963.823594	19.023744
46.321666	1957.688335	19.028762
46.481742	1958.120743	19.033779
46.562132	1971.789877	19.038797
46.555260	1951.319681	19.043815
46.860147	1967.919300	19.048832
46.795006	1960.293747	19.053850
46.520259	1958.914753	19.058867
46.292228	1962.675901	19.063885
46.571506	1953.480214	19.068903
46.558839	1958.856378	19.073920
46.644263	1982.442701	19.078938
46.614185	1987.722549	19.083955
46.484775	1999.479147	19.088973
46.825116	1990.750658	19.093991
46.768528	2006.052915	19.099008
46.572863	1998.893354	19.104026
47.038246	1991.625735	19.109043
46.909851	2008.224172	19.114061
46.744165	2001.576530	19.119079
47.036695	2001.970123	19.124096
47.172712	2016.048759	19.129114
47.077016	2018.351983	19.134131
47.531165	2029.383100	19.139149
47.772635	2021.172652	19.144167
47.762018	2008.609058	19.149184
47.809996	1988.449400	19.154202
48.072236	1977.161071	19.159219
47.878910	1973.632041	19.164237
48.178750	1976.031098	19.169255
47.845505	1971.571751	19.174272
47.312613	1966.722609	19.179290
47.955867	1970.512394	19.184307
47.623641	1975.036746	19.189325
47.631942	1968.261557	19.194343
47.527508	1969.608448	19.199360
47.646356	1975.090822	19.204378
47.914241	1970.559692	19.209395
48.112372	1975.859101	19.214413
47.887513	1976.406298	19.219431
48.112759	1978.741903	19.224448
48.037777	1990.013566	19.229466
48.392774	1996.246602	19.234483
48.261440	1998.636413	19.239501
48.442954	1995.618797	19.244519
48.484233	1991.351659	19.249536
48.245906	1996.352573	19.254554
48.312523	2001.225150	19.259571
48.382209	1995.705025	19.264589
48.376953	1998.145646	19.269607
48.558629	1981.166711	19.274624
48.366300	1999.573739	19.279642
48.428109	1984.775401	19.284659
48.679558	1993.823672	19.289677
48.493954	1989.281660	19.294695
48.511677	1989.283114	19.299712
48.257416	1999.128662	19.304730
48.777398	1996.546202	19.309747
48.730020	2026.124373	19.314765
48.882906	2029.160847	19.319783
49.074721	2030.155079	19.324800
48.780321	2025.533014	19.329818
49.028862	2021.443405	19.334835
49.123745	2025.596828	19.339853
49.264982	2025.548347	19.344871
48.990655	2028.313527	19.349888
49.006980	2035.378842	19.354906
49.257857	2025.676836	19.359923
48.980216	2024.850028	19.364941
49.099544	2027.054340	19.369959
49.519661	2044.678787	19.374976
49.431628	2051.160434	19.379994
49.835386	2051.305160	19.385011
49.842977	2047.997805	19.390029
49.646922	2051.950914	19.395047
49.817161	2041.775266	19.400064
49.677017	2057.829692	19.405082
49.370729	2047.611147	19.410099
49.502363	2047.120795	19.415117
49.838635	2041.695560	19.420135
49.857946	2062.898693	19.425152
49.700677	2075.392948	19.430170
49.960793	2078.969923	19.435187
50.102326	2079.112515	19.440205
50.137570	2075.217179	19.445223
50.367353	2074.511808	19.450240
50.412445	2077.706446	19.455258
50.459734	2071.351497	19.460275
50.426774	2080.996960	19.465293
50.384378	2072.401549	19.470311
50.730482	2073.932828	19.475328
50.469270	2079.471157	19.480346
50.649405	2077.430426	19.485363
50.721048	2069.744029	19.490381
50.707166	2072.175065	19.495399
51.000502	2065.296437	19.500416
50.622241	2067.147990	19.505434
50.955681	2066.495167	19.510451
50.763671	2069.421733	19.515469
50.912514	2081.137725	19.520487
50.616812	2079.280538	19.525504
50.434065	2090.662200	19.530522
50.895601	2095.777388	19.535539
51.033549	2108.691538	19.540557
51.290002	2110.484068	19.545575
51.275786	2110.390613	19.550592
51.112527	2111.702754	19.555610
51.750975	2093.607568	19.560627
51.368781	2106.040602	19.565645
51.344973	2104.690394	19.570663
51.510051	2102.816108	19.575680
51.220981	2105.901226	19.580698
51.606908	2098.456156	19.585715
51.501134	2111.400546	19.590733
51.837489	2128.983622	19.595751
52.031827	2128.392757	19.600768
51.624242	2118.686525	19.605786
51.896106	2130.466271	19.610803
51.881774	2134.218127	19.615821
51.997658	2134.784996	19.620839
52.311626	2132.696160	19.625856
52.133356	2120.543410	19.630874
51.917205	2127.188767	19.635891
52.197275	2128.768952	19.640909
52.201411	2131.653668	19.645927
52.254968	2124.255244	19.650944
52.012524	2127.671604	19.655962
52.318339	2129.960653	19.660979
51.917865	2125.907607	19.665997
51.983892	2137.258231	19.671015
52.391576	2120.298679	19.676032
52.356904	2121.053994	19.681050
52.469353	2134.002690	19.686067
52.255403	2142.096366	19.691085
52.356447	2148.721397	19.696103
52.555014	2142.521914	19.701120
52.490724	2147.638590	19.706138
52.625231	2140.405504	19.711155
52.862551	2137.855167	19.716173
52.652313	2150.053935	19.721191
53.075058	2157.170636	19.726208
52.793474	2169.006639	19.731226
53.196650	2168.290128	19.736243
53.447380	2167.754109	19.741261
53.004261	2186.679726	19.746279
53.221203	2172.260259	19.751296
53.352898	2169.767526	19.756314
53.649498	2158.109248	19.761331
53.315348	2171.272906	19.766349
53.315277	2175.109416	19.771367
53.288856	2161.926320	19.776384
53.086586	2168.910509	19.781402
53.464174	2177.935288	19.786419
53.441863	2181.653045	19.791437
53.575639	2200.093617	19.796455
53.633733	2197.625049	19.801472
53.482594	2203.857961	19.806490
53.602089	2202.623617	19.811507
53.949507	2205.364421	19.816525
53.904797	2229.143870	19.821543
54.740394	2220.514102	19.826560
54.377431	2203.162962	19.831578
54.288213	2193.572165	19.836595
54.575045	2193.525409	19.841613
54.394071	2188.496398	19.846631
54.538026	2179.553036	19.851648
54.742715	2183.540338	19.856666
54.679400	2183.350676	19.861683
54.871685	2190.660581	19.866701
54.662595	2189.632886	19.871719
54.706496	2178.364352	19.876736
54.898600	2191.212343	19.881754
54.773177	2188.306037	19.886771
54.822148	2186.422388	19.891789
54.578774	2196.186938	19.896807
54.606359	2183.481272	19.901824
55.009071	2195.277039	19.906842
54.930238	2205.520262	19.911859
55.300745	2203.587610	19.916877
54.716853	2222.223767	19.921895
54.925599	2211.133657	19.926912
54.946598	2213.190481	19.931930
55.097250	2218.184661	19.936947
55.167087	2217.863556	19.941965
55.201285	2215.554629	19.946983
55.350891	2207.139599	19.952000
55.340468	2215.177043	19.957018
55.354214	2223.916732	19.962035
55.761068	2242.998386	19.967053
55.419848	2246.452943	19.972071
55.769092	2244.996394	19.977088
55.632465	2248.538784	19.982106
55.778027	2231.098853	19.987123
55.904525	2233.293940	19.992141
56.213290	2243.564073	19.997159
56.204125	2236.615684	20.002176
55.982838	2237.475262	20.007194
56.005792	2238.167325	20.012211
56.310949	2234.125976	20.017229
55.940690	2246.804372	20.022247
56.278210	2237.433947	20.027264
56.390324	2234.944242	20.032282
56.437930	2231.142682	20.037299
56.220999	2234.972527	20.042317
56.388962	2235.272550	20.047335
56.535323	2238.316639	20.052352
56.316376	2232.122540	20.057370
56.164346	2238.106029	20.062387
56.664558	2261.367761	20.067405
56.334627	2262.707851	20.072423
56.858391	2269.107383	20.077440
56.767710	2268.269742	20.082458
56.715043	2265.345297	20.087475
57.147762	2262.628410	20.092493
57.077048	2261.364870	20.097511
57.014820	2262.239302	20.102528
56.862296	2254.615052	20.107546
56.793382	2266.097903	20.112563
56.976766	2279.083223	20.117581
56.933805	2290.959799	20.122599
57.158012	2289.305227	20.127616
57.414828	2293.432356	20.132634
57.486357	2299.640713	20.137651
57.532799	2285.639243	20.142669
57.613865	2295.740364	20.147687
57.531628	2293.275484	20.152704
57.917623	2291.649880	20.157722
57.832072	2291.015309	20.162739
58.018555	2281.920188	20.167757
57.961173	2278.321382	20.172775
57.902336	2279.161596	20.177792
57.785530	2295.417315	20.182810
58.116306	2301.692468	20.187827
58.548286	2306.959450	20.192845
58.131703	2314.213351	20.197863
58.096885	2303.064418	20.202880
58.244279	2313.956292	20.207898
58.441556	2314.506175	20.212915
58.683385	2314.388319	20.217933
58.598379	2308.619850	20.222951
58.661325	2305.821358	20.227968
58.988499	2305.115236	20.232986
58.878845	2300.963301	20.238003
59.180416	2300.289557	20.243021
58.930618	2292.343007	20.248039
58.937383	2273.538882	20.253056
58.720354	2274.482396	20.258074
58.773257	2281.637047	20.263091
58.880747	2293.493487	20.268109
59.085429	2290.163156	20.273127
59.014827	2298.778649	20.278144
59.135015	2294.745609	20.283162
59.014123	2294.700095	20.288179
59.375289	2295.129595	20.293197
58.980760	2291.455410	20.298215
59.259900	2296.057548	20.303232
59.580363	2289.889827	20.308250
59.529763	2299.463348	20.313267
59.495573	2294.700374	20.318285
59.212637	2305.698785	20.323303
59.418586	2313.687337	20.328320
59.752146	2324.681514	20.333338
59.610600	2325.463161	20.338355
59.489783	2320.359013	20.343373
59.290827	2328.690051	20.348391
59.426526	2332.740167	20.353408
59.644400	2337.973452	20.358426
59.563801	2355.356619	20.363443
60.076208	2347.235860	20.368461
60.051224	2353.088172	20.373479
59.928474	2359.684731	20.378496
60.205770	2357.830844	20.383514
59.605929	2373.491721	20.388531
60.345423	2372.380282	20.393549
60.572218	2383.878324	20.398567
60.392704	2389.388303	20.403584
60.795981	2384.877589	20.408602
60.665678	2387.604466	20.413619
61.170117	2368.113308	20.418637
60.774634	2377.362406	20.423655
60.545355	2386.495467	20.428672
61.143970	2369.625734	20.433690
60.855720	2382.131253	20.438707
61.105402	2379.211345	20.443725
60.782966	2372.373714	20.448743
60.996256	2385.034917	20.453760
61.206381	2399.460290	20.458778
61.183388	2410.750438	20.463795
61.340265	2402.811621	20.468813
61.384910	2407.326373	20.473831
61.357367	2399.829221	20.478848
61.677812	2403.743125	20.483866
61.660430	2413.231509	20.488883
61.726683	2398.404090	20.493901
61.822862	2407.303475	20.498919
62.010975	2402.126203	20.503936
62.069057	2399.201736	20.508954
61.686443	2407.611391	20.513971
61.964626	2403.462261	20.518989
62.204050	2409.865538	20.524007
61.851906	2409.114990	20.529024
62.155353	2405.289218	20.534042
61.789122	2402.594502	20.539059
62.005113	2412.759420	20.544077
62.294218	2435.608896	20.549095
62.197182	2433.868037	20.554112
62.550111	2435.942080	20.559130
62.062131	2427.417940	20.564147
62.307474	2421.504097	20.569165
62.706249	2438.175906	20.574183
62.390711	2436.354234	20.579200
62.558360	2439.372997	20.584218
62.439514	2466.052238	20.589235
62.799561	2452.556426	20.594253
63.067197	2465.027823	20.599271
63.063866	2462.476457	20.604288
63.165632	2453.819611	20.609306
63.203607	2456.796426	20.614323
63.017828	2449.303944	20.619341
62.999375	2454.033648	20.624359
63.036061	2448.435357	20.629376
63.393536	2453.035620	20.634394
63.337520	2470.015278	20.639411
63.640072	2462.922566	20.644429
63.614034	2485.684442	20.649447
63.850350	2480.850727	20.654464
64.108388	2467.190475	20.659482
63.881373	2471.450358	20.664499
63.797387	2450.573575	20.669517
63.979598	2456.414716	20.674535
63.859453	2469.748562	20.679552
64.103990	2466.654304	20.684570
64.004065	2475.829620	20.689587
64.026097	2470.581353	20.694605
64.246090	2484.897507	20.699623
64.182392	2477.626157	20.704640
64.270005	2473.027631	20.709658
64.107357	2479.296017	20.714675
64.040872	2475.929558	20.719693
64.451507	2466.502427	20.724711
64.433457	2472.057992	20.729728
64.701054	2473.426315	20.734746
64.594525	2494.680165	20.739763
65.104871	2493.533954	20.744781
64.843187	2497.840515	20.749799
64.825023	2511.543735	20.754816
64.947240	2501.411742	20.759834
65.185857	2512.873481	20.764851
65.495905	2503.839104	20.769869
65.390515	2501.833692	20.774887
65.457716	2500.407587	20.779904
65.653518	2490.444333	20.784922
65.120310	2493.326779	20.789939
65.506825	2491.579228	20.794957
65.489522	2488.343997	20.799975
65.113905	2505.124362	20.804992
65.296586	2489.837688	20.810010
65.332148	2504.606550	20.815027
65.457751	2509.602601	20.820045
65.595195	2496.020515	20.825063
65.656485	2517.588174	20.830080
65.512981	2521.009922	20.835098
65.506195	2520.185172	20.840115
65.644279	2519.032962	20.845133
66.027269	2530.283665	20.850151
66.294371	2544.847386	20.855168
66.486913	2550.991361	20.860186
66.494690	2548.837920	20.865203
66.264506	2549.599583	20.870221
66.388992	2553.419539	20.875239
66.365295	2560.989115	20.880256
66.206253	2554.773765	20.885274
66.110338	2562.179304	20.890291
66.262560	2555.556637	20.895309
66.535666	2566.608217	20.900327
66.592505	2584.391538	20.905344
67.278489	2575.870742	20.910362
67.151291	2577.076182	20.915379
66.865804	2582.189400	20.920397
67.298062	2593.130453	20.925415
67.189918	2579.343619	20.930432
67.490719	2572.680448	20.935450
67.544837	2578.476666	20.940467
67.322109	2577.191570	20.945485
67.643798	2577.324081	20.950503
67.512090	2574.674234	20.955520
67.362239	2560.593149	20.960538
67.665431	2574.714351	20.965555
67.467335	2568.329281	20.970573
67.855913	2562.984979	20.975591
67.385355	2575.575500	20.980608
67.845314	2587.297351	20.985626
67.674956	2599.660736	20.990643
67.752673	2597.776026	20.995661
68.122352	2600.968312	21.000679
67.800891	2602.840064	21.005696
67.950190	2587.889102	21.010714
67.663840	2611.217372	21.015731
68.169298	2614.938564	21.020749
68.130292	2615.235988	21.025767
68.226816	2625.372760	21.030784
68.619180	2619.876840	21.035802
68.713898	2617.916489	21.040819
68.472652	2625.384260	21.045837
68.822564	2619.925077	21.050855
68.557697	2624.419588	21.055872
68.501072	2634.663953	21.060890
69.116043	2642.344745	21.065907
69.207213	2649.589103	21.070925
69.308478	2644.886309	21.075943
69.494432	2641.556242	21.080960
69.701166	2639.761027	21.085978
69.529769	2636.945692	21.090995
69.847820	2641.799559	21.096013
69.571073	2636.377002	21.101031
69.782468	2632.145548	21.106048
69.638389	2638.027883	21.111066
69.968703	2622.546614	21.116083
69.609130	2628.722020	21.121101
69.996442	2632.958770	21.126119
69.710353	2633.873563	21.131136
69.879196	2637.804903	21.136154
69.769666	2642.067858	21.141171
69.671612	2634.684993	21.146189
69.933796	2631.027587	21.151207
69.752213	2633.755304	21.156224
69.938021	2658.403364	21.161242
70.162471	2669.965389	21.166259
70.266876	2669.120486	21.171277
70.812762	2656.581323	21.176295
70.341767	2667.270932	21.181312
70.583443	2666.452554	21.186330
70.683662	2668.122356	21.191347
70.605152	2668.932773	21.196365
70.889758	2673.576640	21.201383
70.781318	2698.359012	21.206400
71.067747	2701.995955	21.211418
70.916572	2698.051352	21.216435
70.976045	2698.765745	21.221453
71.519650	2693.834730	21.226471
71.073640	2690.114431	21.231488
71.122834	2691.888331	21.236506
71.124424	2692.090274	21.241523
71.206182	2689.508669	21.246541
71.610153	2703.604674	21.251559
71.748797	2716.287146	21.256576
71.455488	2717.288957	21.261594
71.571055	2720.112064	21.266611
71.575003	2722.005249	21.271629
72.063329	2712.299793	21.276647
71.915288	2710.783262	21.281664
71.852187	2718.235615	21.286682
72.646251	2711.091684	21.291699
72.039557	2712.663362	21.296717
72.257695	2706.994443	21.301735
72.285285	2727.622746	21.306752
72.481162	2743.719200	21.311770
72.858310	2746.775841	21.316787
72.584266	2752.723395	21.321805
72.852134	2747.637941	21.326823
72.652779	2745.544487	21.331840
72.626872	2749.761764	21.336858
73.044223	2738.326784	21.341875
72.669002	2745.070537	21.346893
72.738229	2748.395373	21.351911
72.705674	2749.444642	21.356928
72.947773	2738.898021	21.361946
73.015604	2742.903361	21.366963
72.707857	2749.665885	21.371981
73.190492	2756.085214	21.376999
73.345634	2767.540269	21.382016
73.075811	2765.656084	21.387034
72.920452	2768.844819	21.392051
73.186082	2775.925178	21.397069
73.548200	2782.136887	21.402087
73.653986	2797.228657	21.407104
73.829381	2797.460538	21.412122
73.890492	2800.481231	21.417139
73.820216	2789.611414	21.422157
74.195444	2804.355532	21.427175
74.513916	2797.258266	21.432192
73.859029	2791.281247	21.437210
74.325333	2797.244657	21.442227
74.510071	2793.370890	21.447245
74.892230	2784.694689	21.452263
74.785959	2791.033407	21.457280
74.336970	2785.911686	21.462298
74.686323	2791.527511	21.467315
74.812494	2798.705332	21.472333
74.834951	2806.692771	21.477351
74.747186	2811.154526	21.482368
74.851052	2819.903674	21.487386
75.142387	2814.363164	21.492403
74.740791	2814.480562	21.497421
74.960902	2816.355753	21.502439
75.211382	2820.073858	21.507456
75.185656	2817.157256	21.512474
75.268105	2826.134738	21.517491
75.172847	2838.917376	21.522509
75.230474	2836.528701	21.527527
75.108640	2843.636901	21.532544
75.170490	2850.802148	21.537562
75.889400	2856.413617	21.542579
75.742316	2873.540847	21.547597
75.865445	2879.268099	21.552615
76.436683	2875.563109	21.557632
75.696536	2876.560822	21.562650
76.188378	2878.615515	21.567667
76.276046	2885.108828	21.572685
76.298782	2880.230760	21.577703
76.468103	2876.748871	21.582720
76.117829	2862.432534	21.587738
76.603820	2865.855445	21.592755
76.491797	2880.428987	21.597773
76.466410	2889.123552	21.602791
77.037334	2895.150416	21.607808
76.904493	2895.960375	21.612826
77.183096	2901.101735	21.617843
76.920307	2898.758913	21.622861
77.046932	2904.933213	21.627879
77.467328	2902.459385	21.632896
77.191336	2904.328776	21.637914
77.419201	2892.386046	21.642931
77.269711	2898.002064	21.647949
77.257911	2890.575888	21.652967
77.580102	2892.688144	21.657984
77.188086	2904.923449	21.663002
77.293701	2899.378954	21.668019
77.420013	2920.863206	21.673037
77.320994	2915.255283	21.678055
77.840324	2914.911064	21.683072
77.498134	2920.564840	21.688090
78.046214	2901.706914	21.693107
77.966781	2921.937040	21.698125
78.219597	2936.958982	21.703143
78.417151	2935.528620	21.708160
78.283468	2953.247789	21.713178
78.264122	2942.258036	21.718195
78.510872	2948.126689	21.723213
78.288069	2941.987268	21.728231
78.360521	2942.821570	21.733248
78.449424	2953.826706	21.738266
78.584374	2957.598973	21.743283
78.569470	2974.496213	21.748301
78.392034	2969.013034	21.753319
79.049960	2967.021181	21.758336
78.626982	2975.433874	21.763354
78.905011	2976.344831	21.768371
79.098140	3000.125925	21.773389
79.061352	3004.875756	21.778407
79.468335	3005.185114	21.783424
79.132056	3006.982987	21.788442
79.693578	2997.916413	21.793459
79.461516	3010.908406	21.798477
79.375645	3025.736413	21.803495
80.030534	3030.267232	21.808512
79.681355	3030.870438	21.813530
80.588702	3026.665007	21.818547
80.643437	3016.536545	21.823565
80.400484	3031.512164	21.828583
80.943571	3019.753456	21.833600
80.761808	3013.165117	21.838618
80.732559	3003.460762	21.843635
80.690242	2988.510764	21.848653
80.451958	2990.030642	21.853671
80.730481	2987.803858	21.858688
81.004069	2996.883705	21.863706
81.218979	3017.658205	21.868723
81.259292	3014.865293	21.873741
80.786164	3002.739117	21.878759
80.744433	3007.161826	21.883776
80.611378	3023.606223	21.888794
80.844360	3016.201738	21.893811
81.059785	3013.382252	21.898829
81.062906	3027.378265	21.903847
81.386333	3030.339908	21.908864
81.428494	3038.945052	21.913882
81.571423	3038.925620	21.918899
81.496678	3043.436863	21.923917
81.482092	3052.674596	21.928935
81.559235	3046.084402	21.933952
81.811777	3061.370673	21.938970
81.779241	3065.578896	21.943987
82.165141	3081.250615	21.949005
82.041730	3069.363434	21.954023
82.626311	3065.255817	21.959040
82.252468	3067.645315	21.964058
82.553285	3058.446204	21.969075
82.599578	3065.895213	21.974093
82.824000	3069.230691	21.979111
82.800132	3063.018191	21.984128
82.549735	3077.462034	21.989146
82.736218	3073.350517	21.994163
83.223377	3088.114992	21.999181
82.759561	3084.365650	22.004199
83.316539	3090.336236	22.009216
82.989327	3096.891898	22.014234
83.237304	3094.369763	22.019251
83.480219	3093.296838	22.024269
83.091649	3092.792029	22.029287
83.381579	3086.211141	22.034304
83.220423	3088.119056	22.039322
83.448623	3090.516153	22.044339
83.663696	3100.519084	22.049357
83.604286	3116.730945	22.054375
83.664042	3110.324692	22.059392
83.802599	3121.239068	22.064410
83.804049	3123.568133	22.069427
83.855787	3125.002304	22.074445
83.953890	3121.753776	22.079463
84.107910	3128.543303	22.084480
83.967173	3147.372484	22.089498
84.274344	3152.958405	22.094515
84.295781	3156.431773	22.099533
84.030890	3142.420741	22.104551
84.750680	3163.665924	22.109568
84.755052	3177.999257	22.114586
84.986666	3178.258075	22.119603
85.119428	3173.546767	22.124621
84.546469	3185.835419	22.129639
85.059254	3181.881364	22.134656
85.107218	3185.683416	22.139674
84.996233	3180.489959	22.144691
85.207065	3205.379039	22.149709
85.242001	3211.371769	22.154727
85.554305	3203.758817	22.159744
85.502884	3209.939040	22.164762
85.433211	3210.112217	22.169779
85.865413	3210.043802	22.174797
85.745706	3236.091851	22.179815
86.054676	3230.023097	22.184832
86.265721	3224.916564	22.189850
85.931661	3238.966912	22.194867
86.397883	3225.801499	22.199885
86.211918	3237.056977	22.204903
86.675950	3229.603975	22.209920
86.505751	3220.320796	22.214938
86.792508	3217.598144	22.219955
87.071042	3217.445677	22.224973
86.938345	3226.480596	22.229991
87.219802	3212.646139	22.235008
86.825097	3216.477649	22.240026
87.006982	3216.469889	22.245043
87.463446	3234.365867	22.250061
86.989091	3253.427467	22.255079
87.545345	3244.563191	22.260096
87.290280	3255.381294	22.265114
87.365213	3255.812457	22.270131
87.699951	3262.873747	22.275149
87.443959	3256.748739	22.280167
87.638350	3249.598153	22.285184
87.727414	3253.507205	22.290202
87.454111	3245.054415	22.295219
87.722997	3263.507393	22.300237
87.969869	3270.328488	22.305255
88.176956	3274.732991	22.310272
87.966280	3287.530741	22.315290
88.390259	3276.637960	22.320307
88.383207	3273.661495	22.325325
87.764979	3290.869402	22.330343
88.673183	3307.765247	22.335360
88.495045	3301.095085	22.340378
88.856112	3301.130943	22.345395
89.023636	3308.208074	22.350413
89.163583	3302.665243	22.355431
88.984580	3299.380582	22.360448
89.257546	3310.699643	22.365466
89.032851	3310.117352	22.370483
89.085295	3299.793813	22.375501
89.333877	3312.801906	22.380519
89.385566	3314.471530	22.385536
89.242895	3319.313756	22.390554
89.246323	3324.388528	22.395571
89.697482	3315.713622	22.400589
89.606313	3324.364185	22.405607
89.740141	3330.487073	22.410624
89.790111	3344.652793	22.415642
89.976721	3353.123614	22.420659
90.299803	3357.273150	22.425677
90.115229	3355.566926	22.430695
90.183719	3353.955889	22.435712
90.100743	3342.694088	22.440730
90.158880	3349.911360	22.445747
90.621643	3366.412383	22.450765
90.424454	3376.321416	22.455783
91.116734	3378.026134	22.460800
91.073433	3374.293842	22.465818
91.057531	3372.282583	22.470835
90.916356	3373.898653	22.475853
90.962184	3379.663274	22.480871
91.073058	3377.173593	22.485888
91.123051	3396.090847	22.490906
90.924774	3415.305051	22.495923
91.460802	3412.856524	22.500941
91.523149	3402.366716	22.505959
91.624334	3397.805044	22.510976
91.793840	3406.988946	22.515994
92.020452	3428.242370	22.521011
91.967241	3421.336554	22.526029
91.970140	3434.234169	22.531047
92.444668	3430.684400	22.536064
92.274813	3431.081217	22.541082
92.396491	3435.993967	22.546099
92.656575	3425.040766	22.551117
92.819182	3426.012162	22.556135
92.327780	3422.379103	22.561152
92.215534	3433.128848	22.566170
92.620801	3445.337549	22.571187
92.839576	3452.144471	22.576205
92.681125	3462.862108	22.581223
93.024740	3454.574183	22.586240
93.095013	3458.400961	22.591258
93.066370	3471.866017	22.596275
93.492049	3471.657737	22.601293
93.360517	3493.759401	22.606311
93.589484	3479.220790	22.611328
93.771319	3484.723608	22.616346
93.740956	3483.403299	22.621363
93.991461	3478.829134	22.626381
94.058449	3485.560759	22.631399
94.153737	3475.737105	22.636416
94.403608	3469.891408	22.641434
94.316671	3475.954378	22.646451
94.475872	3469.166195	22.651469
94.174017	3485.131106	22.656487
94.372415	3494.256348	22.661504
94.487628	3499.073731	22.666522
94.773361	3509.888471	22.671539
94.619799	3500.912214	22.676557
94.917170	3514.994688	22.681575
94.952644	3510.762343	22.686592
95.032414	3509.135646	22.691610
95.015384	3505.483233	22.696627
95.261196	3513.925462	22.701645
95.287099	3532.811037	22.706663
95.517211	3529.623680	22.711680
95.539598	3535.967425	22.716698
95.378081	3532.183765	22.721715
95.660062	3540.069248	22.726733
95.211995	3536.975847	22.731751
95.239273	3537.663710	22.736768
95.782068	3548.435999	22.741786
95.854406	3562.376963	22.746803
95.856935	3561.635460	22.751821
95.787126	3570.783021	22.756839
96.318534	3583.813897	22.761856
96.358220	3582.454052	22.766874
96.055219	3596.959430	22.771891
96.450196	3584.250762	22.776909
96.775786	3594.829055	22.781927
96.703251	3593.429092	22.786944
96.758342	3601.435564	22.791962
96.871310	3621.942288	22.796979
96.756544	3618.477258	22.801997
97.115360	3617.322942	22.807015
97.250261	3629.966229	22.812032
97.769216	3618.635863	22.817050
97.452067	3628.568029	22.822067
97.757708	3626.935886	22.827085
97.819079	3631.011815	22.832103
97.947776	3643.483698	22.837120
98.280553	3638.710064	22.842138
97.786384	3644.828977	22.847155
98.382746	3643.375170	22.852173
98.393218	3640.170936	22.857191
98.386053	3650.447955	22.862208
98.498094	3632.315925	22.867226
98.092812	3645.113449	22.872243
98.345387	3637.573543	22.877261
98.463218	3648.798802	22.882279
98.380139	3664.171445	22.887296
98.949506	3660.065796	22.892314
98.976142	3674.172286	22.897331
99.452972	3663.813810	22.902349
99.336701	3669.007294	22.907367
99.535057	3672.940519	22.912384
99.277890	3655.804906	22.917402
99.241819	3680.044210	22.922419
99.496879	3684.854290	22.927437
99.738678	3683.912219	22.932455
99.780789	3697.387039	22.937472
100.091956	3695.366179	22.942490
100.528445	3696.036822	22.947507
100.461833	3686.776404	22.952525
100.450243	3680.304541	22.957543
100.094569	3680.155691	22.962560
100.547201	3680.778784	22.967578
100.534619	3692.401610	22.972595
100.803433	3685.310573	22.977613
100.668701	3692.308693	22.982631
100.740286	3704.044392	22.987648
101.184924	3707.208973	22.992666
100.838765	3715.137714	22.997683
101.287652	3723.831147	23.002701
101.026335	3709.947357	23.007719
100.980754	3709.983879	23.012736
101.190005	3710.175930	23.017754
101.048310	3721.661451	23.022771
101.374358	3723.103105	23.027789
101.571135	3731.347650	23.032807
101.487060	3734.664959	23.037824
102.270044	3734.624013	23.042842
101.881992	3732.312785	23.047859
101.558641	3725.942814	23.052877
101.994160	3745.480649	23.057895
101.675401	3756.405294	23.062912
101.792313	3763.921709	23.067930
101.713809	3770.923172	23.072947
102.068579	3778.946356	23.077965
102.173686	3789.193891	23.082983
102.367994	3793.680576	23.088000
102.793932	3811.783057	23.093018
102.764069	3814.170943	23.098035
103.001448	3818.176498	23.103053
103.618033	3818.337854	23.108071
103.602327	3814.113884	23.113088
103.365740	3809.502394	23.118106
103.554474	3806.482844	23.123123
103.326894	3808.646313	23.128141
103.851220	3822.073446	23.133159
103.893317	3832.539692	23.138176
103.804545	3830.047102	23.143194
103.949084	3848.359119	23.148211
103.859275	3844.726921	23.153229
104.090679	3838.481770	23.158247
103.814566	3851.955765	23.163264
104.134522	3854.658691	23.168282
104.450093	3872.462547	23.173299
104.358952	3859.999341	23.178317
104.958945	3868.554498	23.183335
104.788877	3872.446291	23.188352
104.936915	3867.588153	23.193370
104.984683	3886.214241	23.198387
105.222829	3893.530762	23.203405
105.558037	3886.372363	23.208423
105.315102	3889.299809	23.213440
105.377879	3885.186867	23.218458
105.739293	3881.561201	23.223475
105.665371	3893.264393	23.228493
105.847242	3884.373039	23.233511
106.082626	3910.714334	23.238528
106.305244	3907.256087	23.243546
106.345004	3923.178775	23.248563
106.475436	3915.321905	23.253581
106.350006	3911.729436	23.258599
106.300450	3918.424601	23.263616
106.601266	3912.480949	23.268634
106.426527	3918.023159	23.273651
106.320823	3917.090466	23.278669
106.519880	3931.463192	23.283687
106.229545	3944.938829	23.288704
106.674231	3942.309644	23.293722
106.783723	3954.213286	23.298739
107.204775	3958.834208	23.303757
107.246955	3969.335178	23.308775
107.644546	3983.339705	23.313792
107.734247	3987.734675	23.318810
107.733017	3966.363424	23.323827
107.739073	3980.700764	23.328845
107.671633	3980.986573	23.333863
107.793053	4002.581008	23.338880
107.816240	3993.994166	23.343898
108.455766	3999.311298	23.348915
108.533376	4002.402729	23.353933
108.715011	3991.797928	23.358951
108.374656	4010.694212	23.363968
108.424962	4009.680614	23.368986
109.071666	4017.847419	23.374003
108.615191	4022.652738	23.379021
109.147049	4028.361697	23.384039
108.819148	4028.386602	23.389056
109.027974	4030.992173	23.394074
109.037647	4027.723816	23.399091
109.161775	4046.014636	23.404109
109.583589	4038.161524	23.409127
109.369270	4052.929844	23.414144
109.869655	4047.133483	23.419162
109.659942	4048.222350	23.424179
109.492954	4049.673459	23.429197
110.015723	4050.650737	23.434215
110.357448	4068.733575	23.439232
110.397815	4088.364305	23.444250
110.519123	4071.359792	23.449267
110.756000	4084.600395	23.454285
110.809642	4068.641348	23.459303
110.435733	4070.400280	23.464320
110.716181	4077.615801	23.469338
111.021954	4076.458013	23.474355
110.698986	4095.490506	23.479373
110.903716	4099.359005	23.484391
111.046683	4108.414240	23.489408
111.224643	4106.094465	23.494426
111.499586	4109.528517	23.499443
111.351814	4142.175042	23.504461
111.490311	4128.006299	23.509479
111.828687	4141.754211	23.514496
111.984510	4137.075811	23.519514
111.946428	4137.554809	23.524531
111.592858	4154.444726	23.529549
112.405194	4152.924083	23.534567
112.199100	4164.159933	23.539584
112.055626	4160.297544	23.544602
112.172112	4170.066269	23.549619
112.162690	4189.665589	23.554637
112.425495	4188.994437	23.559655
112.727135	4200.326735	23.564672
113.134516	4214.195990	23.569690
113.007678	4222.462380	23.574707
113.057902	4226.682438	23.579725
113.363219	4224.786106	23.584743
113.219766	4223.602536	23.589760
113.452169	4246.658158	23.594778
113.646259	4245.592045	23.599795
113.550166	4254.184486	23.604813
114.023674	4249.080315	23.609831
113.798719	4250.597715	23.614848
114.239640	4273.965786	23.619866
114.341914	4275.113749	23.624883
114.330854	4284.271706	23.629901
114.453077	4270.031899	23.634919
114.545593	4277.189194	23.639936
114.583868	4283.559360	23.644954
114.963777	4303.157483	23.649971
114.980378	4311.730940	23.654989
115.268830	4316.245923	23.660007
115.174241	4305.326697	23.665024
115.041074	4305.628097	23.670042
115.233140	4315.289932	23.675059
115.475742	4330.556657	23.680077
115.543579	4334.099395	23.685095
116.184193	4334.462312	23.690112
116.095304	4335.968261	23.695130
116.111216	4339.840461	23.700147
116.041502	4339.578203	23.705165
116.168447	4335.738017	23.710183
116.161288	4352.068914	23.715200
116.498501	4361.210313	23.720218
116.714810	4361.589012	23.725235
116.360123	4368.826546	23.730253
116.717362	4365.178624	23.735271
116.892343	4366.264577	23.740288
116.660294	4363.685336	23.745306
117.101633	4371.912644	23.750323
116.777611	4393.959199	23.755341
117.029509	4382.698398	23.760359
116.680652	4408.068523	23.765376
117.336996	4416.837127	23.770394
117.424695	4422.837354	23.775411
117.166567	4434.878099	23.780429
117.427338	4435.226223	23.785447
117.890157	4444.737881	23.790464
117.715572	4464.230185	23.795482
118.281387	4467.359940	23.800499
118.400841	4490.670034	23.805517
118.873938	4482.697985	23.810535
118.714057	4483.898732	23.815552
118.970079	4481.552617	23.820570
118.727452	4483.507628	23.825587
119.073133	4494.027701	23.830605
119.478506	4500.592822	23.835623
119.291149	4501.296902	23.840640
119.814483	4499.868082	23.845658
119.893761	4503.631028	23.850675
119.903962	4499.722687	23.855693
119.885832	4504.751797	23.860711
119.980799	4503.731969	23.865728
119.744098	4501.652319	23.870746
120.362592	4494.386593	23.875763
120.102381	4493.938476	23.880781
120.459205	4516.143579	23.885799
120.710337	4522.964523	23.890816
120.756223	4524.028117	23.895834
121.048912	4525.967515	23.900851
121.132441	4517.227098	23.905869
120.795151	4517.400806	23.910887
121.054087	4516.866509	23.915904
121.088000	4517.241885	23.920922
121.372645	4536.157580	23.925939
121.631326	4549.096140	23.930957
121.874718	4558.551996	23.935975
121.956094	4557.223762	23.940992
121.716175	4549.962054	23.946010
121.877398	4550.519949	23.951027
121.798661	4548.445688	23.956045
122.064280	4564.915602	23.961063
122.430893	4579.793554	23.966080
122.351999	4584.021659	23.971098
122.402157	4589.461978	23.976115
122.047502	4582.114484	23.981133
122.353905	4594.234912	23.986151
123.004204	4600.545810	23.991168
122.806507	4610.849828	23.996186
123.164657	4605.044088	24.001203
122.889078	4620.693592	24.006221
123.401185	4620.813957	24.011239
123.501682	4629.289469	24.016256
123.223499	4645.533953	24.021274
123.723935	4628.712658	24.026291
124.062272	4655.162619	24.031309
123.983917	4657.615343	24.036327
124.153798	4658.302529	24.041344
124.161350	4662.555349	24.046362
124.410777	4649.789942	24.051379
124.408983	4661.981824	24.056397
124.260279	4670.175287	24.061415
124.505089	4681.477561	24.066432
124.728179	4694.096905	24.071450
124.871630	4685.681554	24.076467
124.918089	4690.505550	24.081485
125.021142	4698.141644	24.086503
125.347035	4708.505674	24.091520
125.116964	4717.592195	24.096538
125.427283	4712.458537	24.101555
125.515748	4721.772364	24.106573
125.603633	4736.275629	24.111591
125.903691	4743.977625	24.116608
126.136389	4750.976925	24.121626
126.004327	4747.357403	24.126643
126.295428	4745.972449	24.131661
126.197265	4754.020587	24.136679
126.534873	4761.477787	24.141696
126.273486	4783.861416	24.146714
126.779247	4768.878201	24.151731
126.908441	4774.887456	24.156749
126.649910	4792.622654	24.161767
127.190059	4803.250971	24.166784
127.123755	4813.930291	24.171802
127.513776	4803.891731	24.176819
127.493163	4819.862322	24.181837
127.948195	4835.790162	24.186855
128.162841	4828.337453	24.191872
128.124886	4830.211833	24.196890
128.049090	4832.454303	24.201907
128.128372	4837.494985	24.206925
128.441043	4830.561158	24.211943
128.456827	4855.055157	24.216960
128.633670	4872.168460	24.221978
128.704217	4865.549451	24.226995
128.661082	4859.794177	24.232013
128.603141	4876.632085	24.237031
129.204721	4885.467490	24.242048
129.255088	4895.542501	24.247066
129.186751	4894.621292	24.252083
129.372021	4888.274284	24.257101
129.286081	4907.642248	24.262119
129.703840	4912.869563	24.267136
130.023107	4918.127329	24.272154
130.131336	4917.927003	24.277171
130.194859	4922.430115	24.282189
130.412207	4940.567987	24.287207
130.537314	4938.412349	24.292224
130.358070	4944.679741	24.297242
130.601903	4938.806934	24.302259
130.797220	4937.985080	24.307277
130.869196	4970.212740	24.312295
131.207529	4961.905208	24.317312
131.253484	4982.815381	24.322330
131.414982	4964.299191	24.327347
131.404750	4968.371159	24.332365
131.624156	4986.106348	24.337383
132.221054	4995.509568	24.342400
131.855634	5003.801620	24.347418
131.717166	4991.211459	24.352435
132.128829	5000.738212	24.357453
131.607831	5003.794100	24.362471
132.229299	5020.970723	24.367488
131.903353	5032.486472	24.372506
132.108074	5035.769722	24.377523
132.758564	5046.957190	24.382541
132.474946	5065.189799	24.387559
132.862454	5059.774352	24.392576
132.747838	5077.267174	24.397594
132.971675	5089.409112	24.402611
133.138284	5089.641698	24.407629
132.988993	5101.266115	24.412647
133.810897	5099.607970	24.417664
133.913264	5110.685644	24.422682
133.829030	5107.038054	24.427699
134.189329	5107.905232	24.432717
134.026375	5115.016930	24.437735
134.494739	5124.177269	24.442752
134.134811	5146.001659	24.447770
134.420095	5140.525904	24.452787
135.017993	5142.206266	24.457805
134.517634	5144.298050	24.462823
134.694693	5153.752235	24.467840
135.304185	5160.846953	24.472858
135.177043	5168.911512	24.477875
135.589005	5173.369326	24.482893
135.512564	5171.478478	24.487911
135.884715	5184.713809	24.492928
135.934279	5186.274133	24.497946
135.944598	5188.410289	24.502963
136.457511	5192.157265	24.507981
136.003162	5193.946541	24.512999
136.288716	5196.046275	24.518016
136.309973	5211.611094	24.523034
136.390742	5227.489357	24.528051
136.763247	5227.584369	24.533069
136.684885	5233.389491	24.538087
136.861929	5251.169386	24.543104
137.174983	5256.286941	24.548122
137.108728	5261.621128	24.553139
137.513812	5269.965941	24.558157
137.367482	5290.663392	24.563175
137.454330	5282.649635	24.568192
137.291156	5299.186848	24.573210
137.473427	5309.366720	24.578227
137.924686	5313.658222	24.583245
138.099013	5324.065819	24.588263
138.342298	5338.988895	24.593280
138.291930	5354.401501	24.598298
138.681287	5358.652451	24.603315
139.208073	5361.658119	24.608333
138.843229	5378.629571	24.613351
139.224946	5380.575236	24.618368
139.249423	5377.697895	24.623386
139.729898	5375.709879	24.628403
139.332247	5388.289034	24.633421
139.195489	5399.109542	24.638439
139.884663	5409.495516	24.643456
140.257578	5408.022569	24.648474
140.210810	5410.480429	24.653491
140.333570	5413.326859	24.658509
140.168804	5434.026758	24.663527
140.430606	5442.761917	24.668544
140.514967	5436.603823	24.673562
140.258740	5441.882050	24.678579
140.839601	5460.151032	24.683597
140.738618	5470.226222	24.688615
141.223483	5476.913677	24.693632
141.552433	5496.737496	24.698650
141.510061	5503.704232	24.703667
141.526120	5497.304615	24.708685
141.748534	5507.631546	24.713703
142.005173	5493.551114	24.718720
141.961683	5512.585607	24.723738
141.979570	5531.184340	24.728755
142.359427	5520.158697	24.733773
142.230234	5525.098994	24.738791
142.663026	5530.898513	24.743808
142.640117	5554.176624	24.748826
142.622816	5550.446995	24.753843
142.854915	5553.123397	24.758861
142.931441	5557.242607	24.763879
143.102627	5565.715215	24.768896
143.418588	5579.052696	24.773914
143.501267	5576.562602	24.778931
143.686487	5580.050790	24.783949
143.892942	5600.360000	24.788967
143.850353	5602.547086	24.793984
144.384803	5602.902780	24.799002
144.397844	5610.173832	24.804019
144.481015	5608.693226	24.809037
144.290600	5621.969517	24.814055
144.350103	5629.699889	24.819072
144.831657	5635.834347	24.824090
144.585361	5644.088938	24.829107
145.029056	5654.922778	24.834125
145.224787	5668.501884	24.839143
144.998839	5672.895938	24.844160
145.552162	5685.835187	24.849178
145.586063	5699.800557	24.854195
145.825665	5696.381246	24.859213
145.725361	5703.508056	24.864231
146.003856	5725.582923	24.869248
146.209810	5734.366849	24.874266
146.367534	5743.611960	24.879283
146.428172	5751.539081	24.884301
146.266376	5765.496289	24.889319
147.070806	5763.600385	24.894336
147.279726	5771.880624	24.899354
147.322722	5786.909674	24.904371
147.751146	5791.527174	24.909389
147.909887	5795.404091	24.914407
147.738825	5787.011770	24.919424
148.000663	5785.336248	24.924442
147.796792	5787.074355	24.929459
148.391748	5802.541420	24.934477
148.395468	5813.560292	24.939495
148.542809	5807.260920	24.944512
148.546122	5813.789870	24.949530
148.564836	5820.445824	24.954547
149.105136	5832.706545	24.959565
149.269803	5841.651706	24.964583
149.457082	5831.655050	24.969600
149.309964	5834.700110	24.974618
149.305580	5843.954347	24.979635
149.475070	5849.900264	24.984653
149.815211	5859.017649	24.989671
149.986606	5869.259535	24.994688
149.986164	5871.744463	24.999706
149.706247	5879.538131	25.004723
150.253004	5905.483262	25.009741
150.149003	5901.290642	25.014759
150.458399	5931.298451	25.019776
150.865685	5930.930176	25.024794
150.656875	5942.062220	25.029811
150.934101	5948.518403	25.034829
151.181482	5959.977107	25.039847
151.457103	5966.950961	25.044864
151.764522	5963.729866	25.049882
151.616625	5977.208517	25.054899
151.986418	5970.611260	25.059917
152.066157	5976.571661	25.064935
152.217769	5988.862868	25.069952
152.185330	5978.860687	25.074970
152.224578	5995.899517	25.079987
152.439092	6013.111009	25.085005
152.481429	6017.168657	25.090023
152.803616	6020.303554	25.095040
152.802091	6008.787355	25.100058
152.974497	6041.760975	25.105075
153.490654	6038.276205	25.110093
153.228316	6036.824300	25.115111
153.358606	6043.917493	25.120128
153.857097	6062.094869	25.125146
153.721658	6063.078277	25.130163
154.130746	6058.715780	25.135181
154.474646	6084.336405	25.140199
154.346635	6090.024044	25.145216
154.688440	6099.668542	25.150234
154.325675	6100.671402	25.155251
154.805805	6102.145315	25.160269
155.007010	6116.704375	25.165287
155.169523	6127.484990	25.170304
155.409896	6127.866060	25.175322
155.334853	6127.512510	25.180339
155.371526	6134.408582	25.185357
155.782519	6153.976332	25.190375
155.966898	6150.940123	25.195392
156.029829	6155.396830	25.200410
156.186551	6175.112938	25.205427
156.403176	6183.388185	25.210445
156.593548	6191.222032	25.215463
156.466981	6191.688150	25.220480
156.899302	6209.109577	25.225498
156.915591	6222.313237	25.230515
156.985404	6222.888662	25.235533
157.319196	6242.127490	25.240551
157.427303	6250.597111	25.245568
157.427064	6248.782926	25.250586
157.382105	6272.432341	25.255603
157.564495	6283.582282	25.260621
158.119327	6304.834614	25.265639
158.167700	6312.995975	25.270656
158.495428	6317.327070	25.275674
158.336658	6319.341295	25.280691
158.938039	6324.491889	25.285709
159.000587	6341.661912	25.290727
159.064980	6335.926130	25.295744
159.417381	6338.787549	25.300762
159.260763	6356.372608	25.305779
159.587758	6366.924599	25.310797
159.970643	6371.960105	25.315815
159.709709	6374.270007	25.320832
160.021791	6399.916881	25.325850
159.863563	6410.683748	25.330867
160.111489	6406.494269	25.335885
160.236827	6431.473504	25.340903
160.253487	6443.476286	25.345920
160.507488	6440.456082	25.350938
161.119858	6466.955183	25.355955
161.339495	6449.608163	25.360973
162.014070	6453.524441	25.365991
162.221792	6460.775925	25.371008
161.839166	6452.424505	25.376026
162.115386	6462.828231	25.381043
162.190413	6480.245207	25.386061
162.488296	6478.733767	25.391079
162.116563	6475.583838	25.396096
162.200540	6481.833547	25.401114
162.630869	6504.532178	25.406131
162.459840	6514.579052	25.411149
162.878696	6521.464121	25.416167
163.006524	6525.595191	25.421184
163.196767	6544.010710	25.426202
162.722202	6553.976244	25.431219
163.220765	6556.286683	25.436237
163.863943	6565.968302	25.441255
163.881377	6586.375782	25.446272
164.014116	6579.236231	25.451290
163.968957	6593.131585	25.456307
164.157289	6614.284236	25.461325
164.368370	6610.546546	25.466343
164.568397	6615.257161	25.471360
164.947440	6628.364993	25.476378
164.862868	6640.048369	25.481395
164.815000	6633.786830	25.486413
164.861650	6658.768401	25.491431
165.262134	6676.739021	25.496448
165.799858	6665.853062	25.501466
165.861299	6697.314602	25.506483
165.736615	6704.173006	25.511501
165.925944	6694.450323	25.516519
166.073061	6732.086380	25.521536
166.487486	6733.727937	25.526554
166.645877	6728.426175	25.531571
166.703931	6758.633820	25.536589
167.315261	6763.121369	25.541607
167.059831	6766.970881	25.546624
167.300705	6763.106160	25.551642
167.451507	6784.307770	25.556659
167.647573	6799.015585	25.561677
168.054525	6795.065923	25.566695
167.740080	6816.346026	25.571712
168.262725	6827.520462	25.576730
168.349704	6825.397252	25.581747
168.274118	6840.860372	25.586765
168.329272	6848.649949	25.591783
168.515743	6867.522468	25.596800
168.912057	6879.693607	25.601818
169.375022	6890.959069	25.606835
168.991478	6896.901076	25.611853
169.511753	6910.237041	25.616871
169.386989	6919.766973	25.621888
169.813986	6922.961916	25.626906
170.104247	6937.169943	25.631923
169.939424	6944.508411	25.636941
170.344732	6958.860474	25.641959
170.244018	6975.843947	25.646976
170.568272	6976.695535	25.651994
171.254650	6990.078154	25.657011
171.403991	7005.359357	25.662029
171.449970	7006.460908	25.667047
171.704694	7005.722857	25.672064
172.184169	7004.115208	25.677082
172.011456	7000.739331	25.682100
171.873786	7028.065825	25.687117
172.099706	7029.791329	25.692135
172.100931	7040.443282	25.697152
172.334284	7055.965826	25.702170
172.620511	7060.170887	25.707188
172.698047	7083.531141	25.712205
172.818537	7072.136555	25.717223
172.843652	7095.273942	25.722240
173.304869	7101.860865	25.727258
173.435826	7116.268643	25.732276
173.537254	7137.107938	25.737293
173.965540	7135.333104	25.742311
173.825156	7144.742891	25.747328
174.167593	7164.982432	25.752346
174.500407	7155.909136	25.757364
174.506216	7168.394686	25.762381
174.706876	7165.780887	25.767399
174.874964	7192.086846	25.772416
175.141997	7186.752803	25.777434
175.562559	7188.227217	25.782452
175.466459	7195.821435	25.787469
175.612360	7194.452391	25.792487
175.739786	7219.799543	25.797504
175.709597	7218.670665	25.802522
175.972471	7221.076855	25.807540
176.109132	7247.914205	25.812557
176.380881	7249.962946	25.817575
176.567356	7251.605997	25.822592
176.558305	7257.236594	25.827610
176.936126	7277.505087	25.832628
176.509772	7281.564897	25.837645
177.268827	7294.527012	25.842663
177.477226	7310.839153	25.847680
177.582685	7314.881193	25.852698
177.960068	7325.122283	25.857716
177.828296	7347.017949	25.862733
178.317609	7344.736830	25.867751
177.976743	7354.940677	25.872768
178.350973	7366.608637	25.877786
179.028089	7380.347535	25.882804
178.844651	7394.007325	25.887821
179.081781	7399.672905	25.892839
179.082064	7407.442683	25.897856
179.204838	7416.378337	25.902874
179.763566	7425.292367	25.907892
179.983743	7435.416164	25.912909
179.895660	7438.999546	25.917927
180.117778	7457.675497	25.922944
180.428911	7458.164626	25.927962
180.779801	7462.266175	25.932980
180.538921	7480.912332	25.937997
180.835372	7491.356714	25.943015
180.730258	7494.248264	25.948032
180.918866	7517.566393	25.953050
181.445083	7521.796506	25.958068
181.088900	7538.598331	25.963085
181.826317	7549.419607	25.968103
182.050074	7550.291772	25.973120
182.039293	7560.459325	25.978138
182.118020	7576.276502	25.983156
182.500120	7599.340677	25.988173
182.556089	7596.803484	25.993191
182.752250	7619.058043	25.998208
182.897575	7625.593420	26.003226
183.214312	7639.788256	26.008244
183.246106	7659.513475	26.013261
183.796868	7662.960633	26.018279
184.179086	7688.724035	26.023296
184.033845	7688.719930	26.028314
184.224674	7687.129980	26.033332
184.515300	7700.344680	26.038349
184.591373	7713.640523	26.043367
184.689472	7722.774966	26.048384
184.947491	7716.915327	26.053402
185.157140	7739.330073	26.058420
185.178415	7750.411588	26.063437
185.434941	7748.731228	26.068455
185.541403	7769.298801	26.073472
185.396619	7789.510172	26.078490
186.349161	7793.033529	26.083508
185.955866	7822.950762	26.088525
186.337762	7818.241794	26.093543
186.420606	7811.222561	26.098560
186.910122	7830.062699	26.103578
187.371696	7833.773517	26.108596
187.199222	7847.729604	26.113613
187.352933	7842.843315	26.118631
187.630993	7850.043651	26.123648
187.675671	7864.137933	26.128666
188.071956	7858.546026	26.133684
187.654627	7880.015469	26.138701
188.354337	7884.001996	26.143719
188.547144	7894.267655	26.148736
188.589599	7906.622503	26.153754
188.688321	7909.549759	26.158772
188.713597	7924.308110	26.163789
188.615856	7929.269951	26.168807
188.851223	7949.279304	26.173824
188.920940	7955.128695	26.178842
188.983483	7983.019982	26.183860
189.264915	7991.980153	26.188877
189.737848	8020.952834	26.193895
189.634436	8042.168996	26.198912
189.942199	8058.965632	26.203930
190.524359	8071.542542	26.208948
190.491142	8094.791058	26.213965
190.511376	8102.661847	26.218983
191.339463	8112.495815	26.224000
190.932725	8128.123603	26.229018
191.914855	8129.805406	26.234036
191.779292	8157.589537	26.239053
192.061526	8158.477279	26.244071
192.274715	8172.828326	26.249088
192.235285	8187.611791	26.254106
192.502958	8185.501075	26.259124
192.546800	8211.240114	26.264141
192.853058	8220.747655	26.269159
193.082613	8234.886545	26.274176
192.597415	8250.778671	26.279194
193.402387	8252.390519	26.284212
193.653659	8280.719000	26.289229
194.030654	8283.462509	26.294247
194.461275	8304.729407	26.299264
194.419140	8308.125024	26.304282
194.805997	8313.648836	26.309300
194.857056	8316.322548	26.314317
195.001243	8334.816291	26.319335
195.547375	8342.783824	26.324352
195.424901	8346.261249	26.329370
195.966268	8355.224361	26.334388
195.817893	8368.891010	26.339405
196.198347	8371.510305	26.344423
195.978393	8371.507516	26.349440
196.241017	8397.967629	26.354458
196.969724	8400.219056	26.359476
197.045737	8404.195354	26.364493
197.274898	8397.390340	26.369511
197.558085	8413.929130	26.374528
197.393351	8429.871665	26.379546
197.490677	8433.484496	26.384564
197.826795	8435.118700	26.389581
198.159794	8457.763765	26.394599
198.640457	8457.342758	26.399616
198.150619	8472.259195	26.404634
198.193774	8472.383063	26.409652
198.379966	8498.436947	26.414669
198.321663	8506.054689	26.419687
198.827229	8520.904368	26.424704
198.950219	8541.666337	26.429722
199.376813	8550.216894	26.434740
199.434941	8567.884710	26.439757
199.528118	8583.373632	26.444775
200.304628	8588.886719	26.449792
200.130096	8601.152725	26.454810
200.339044	8602.309376	26.459828
200.454796	8625.101635	26.464845
200.499013	8629.364434	26.469863
201.299818	8633.355720	26.474880
201.484191	8648.921005	26.479898
201.990361	8648.342975	26.484916
201.791314	8658.317858	26.489933
201.539938	8663.925983	26.494951
201.974334	8672.320150	26.499968
201.666621	8691.926317	26.504986
201.826123	8710.692860	26.510004
202.214106	8721.720764	26.515021
202.458907	8740.559102	26.520039
202.818825	8756.755544	26.525056
202.777668	8780.857046	26.530074
203.362065	8788.357703	26.535092
203.461333	8794.619981	26.540109
203.620675	8808.044762	26.545127
204.054594	8824.830818	26.550144
203.895324	8842.862528	26.555162
204.176240	8857.593686	26.560180
204.293826	8866.913820	26.565197
204.388823	8888.908834	26.570215
204.865587	8907.515279	26.575232
205.044910	8922.754786	26.580250
205.156311	8939.053914	26.585268
205.434168	8941.339746	26.590285
205.704885	8964.821301	26.595303
206.496147	8970.219451	26.600320
205.930135	8977.746445	26.605338
206.500975	9001.653429	26.610356
206.835594	9005.747045	26.615373
206.877318	9019.377330	26.620391
207.220873	9027.812689	26.625408
207.330398	9052.223678	26.630426
207.298559	9064.601942	26.635444
207.588850	9066.891252	26.640461
208.111851	9087.297977	26.645479
208.880343	9094.324115	26.650496
208.846098	9103.482796	26.655514
209.126836	9097.102184	26.660532
209.331625	9103.460574	26.665549
209.400973	9126.006012	26.670567
209.314113	9134.418812	26.675584
209.367254	9134.423672	26.680602
209.391712	9152.024447	26.685620
209.701953	9170.071896	26.690637
209.816263	9198.572729	26.695655
210.089601	9196.700400	26.700672
209.951259	9215.904291	26.705690
210.219568	9234.424259	26.710708
210.741456	9256.529626	26.715725
210.681813	9269.524673	26.720743
210.916459	9284.928677	26.725760
211.216207	9310.419265	26.730778
211.457681	9327.454264	26.735796
212.199492	9331.983229	26.740813
212.228365	9345.130701	26.745831
212.673896	9358.407838	26.750848
212.568042	9368.934901	26.755866
212.429847	9374.500943	26.760884
213.164061	9394.858199	26.765901
213.141860	9410.512713	26.770919
213.761811	9417.523368	26.775936
213.550847	9424.620117	26.780954
213.932153	9434.470449	26.785972
214.172629	9436.898013	26.790989
214.255314	9456.643051	26.796007
214.208270	9451.185281	26.801024
214.587270	9477.304223	26.806042
214.768625	9494.751846	26.811060
215.049931	9502.532931	26.816077
215.003191	9518.327089	26.821095
215.749115	9519.203676	26.826112
215.313351	9541.362120	26.831130
215.414847	9553.521021	26.836148
215.927529	9569.164508	26.841165
215.743210	9589.368943	26.846183
216.462919	9608.256662	26.851200
216.702193	9625.604274	26.856218
216.727914	9635.066070	26.861236
217.018949	9649.505629	26.866253
217.571429	9673.509609	26.871271
217.799490	9681.345266	26.876288
217.892592	9694.409945	26.881306
217.912835	9706.264944	26.886324
218.306696	9711.478524	26.891341
218.055142	9735.520134	26.896359
218.592567	9739.073149	26.901376
218.813940	9772.690799	26.906394
218.994376	9790.738344	26.911412
219.297740	9806.142527	26.916429
219.203210	9825.372207	26.921447
219.629656	9836.940416	26.926464
219.846673	9870.134415	26.931482
219.749605	9873.569375	26.936500
220.384467	9887.883023	26.941517
220.613058	9926.055148	26.946535
220.651480	9940.223987	26.951552
220.937135	9953.565061	26.956570
221.260703	9979.236322	26.961588
221.576525	9989.821731	26.966605
221.782336	9997.528884	26.971623
222.164720	10011.682703	26.976640
222.242802	10019.248700	26.981658
222.574852	10030.156784	26.986676
222.983468	10045.282285	26.991693
222.960709	10051.243041	26.996711
223.275636	10064.625847	27.001728
223.810507	10088.199327	27.006746
223.785744	10089.532558	27.011764
224.104875	10103.254210	27.016781
224.232302	10117.965422	27.021799
224.316722	10123.273590	27.026816
224.499317	10135.506186	27.031834
224.601725	10146.451505	27.036852
225.498819	10165.511450	27.041869
225.311599	10188.819977	27.046887
225.481373	10191.739854	27.051904
225.745944	10214.207311	27.056922
225.682986	10216.570123	27.061940
226.092522	10236.701674	27.066957
226.210499	10256.311895	27.071975
226.427358	10271.398398	27.076992
226.993884	10285.665404	27.082010
227.035430	10300.212946	27.087028
227.645677	10316.577579	27.092045
227.765841	10312.118305	27.097063
228.143367	10339.722208	27.102080
228.333981	10349.232806	27.107098
228.376628	10344.868255	27.112116
228.620598	10352.571638	27.117133
228.638935	10372.586818	27.122151
228.975712	10378.267726	27.127168
229.099640	10387.108759	27.132186
229.157364	10412.433136	27.137204
229.594334	10404.103322	27.142221
229.737156	10425.192168	27.147239
230.162663	10442.376771	27.152256
230.496785	10438.832913	27.157274
230.106589	10451.608615	27.162292
230.792366	10471.547514	27.167309
230.700637	10488.119687	27.172327
230.805764	10496.867783	27.177344
230.944392	10515.053032	27.182362
231.390671	10530.308263	27.187380
231.894402	10544.740275	27.192397
231.698024	10576.166235	27.197415
231.959962	10573.419659	27.202432
232.492343	10592.825542	27.207450
232.820064	10604.574474	27.212468
232.813108	10613.256075	27.217485
233.157818	10626.569049	27.222503
233.382248	10643.930462	27.227520
233.613009	10662.398426	27.232538
233.807116	10682.752833	27.237556
233.751946	10692.791075	27.242573
234.257715	10706.221663	27.247591
234.305935	10733.334743	27.252608
235.281571	10738.378490	27.257626
235.313967	10750.186565	27.262644
235.806540	10760.784248	27.267661
235.987895	10761.024734	27.272679
236.083748	10779.197658	27.277696
236.603533	10772.521653	27.282714
236.770341	10793.365181	27.287732
236.836751	10801.221796	27.292749
237.111279	10811.985520	27.297767
237.046368	10829.755734	27.302784
237.416106	10839.492262	27.307802
237.179506	10856.644123	27.312820
237.803609	10866.920796	27.317837
237.838334	10879.833023	27.322855
237.815087	10900.582050	27.327872
238.370090	10922.308498	27.332890
238.200322	10943.584383	27.337908
238.606042	10967.468825	27.342925
238.933053	10977.598502	27.347943
238.798822	11005.229027	27.352960
239.329273	11022.004606	27.357978
239.404954	11040.566378	27.362996
239.449280	11060.328400	27.368013
239.663874	11083.983842	27.373031
240.058628	11107.403944	27.378048
240.450605	11121.619399	27.383066
240.417708	11153.477174	27.388084
241.039710	11175.578906	27.393101
241.545706	11193.012560	27.398119
241.922737	11212.952194	27.403136
242.182764	11221.907487	27.408154
242.371962	11239.974128	27.413172
242.725341	11257.589836	27.418189
243.229163	11267.305259	27.423207
243.078167	11273.546050	27.428224
243.128653	11289.565376	27.433242
243.136227	11309.284935	27.438260
243.640604	11327.424069	27.443277
243.617202	11339.146475	27.448295
243.748511	11357.259838	27.453312
244.182438	11376.593134	27.458330
244.335938	11403.721463	27.463348
244.749321	11417.455457	27.468365
245.194359	11430.497282	27.473383
245.210651	11441.639694	27.478400
245.936163	11449.375123	27.483418
245.574665	11472.269995	27.488436
245.917500	11480.642178	27.493453
246.296403	11496.323056	27.498471
246.574963	11519.525833	27.503488
246.888578	11528.258952	27.508506
247.062887	11548.454655	27.513524
247.065833	11548.199961	27.518541
247.535032	11575.422949	27.523559
247.398258	11598.914259	27.528576
247.580354	11615.933938	27.533594
248.008827	11629.174035	27.538612
248.358624	11660.379524	27.543629
248.592071	11670.339966	27.548647
248.736542	11697.101592	27.553664
249.103325	11711.356397	27.558682
249.250364	11733.431022	27.563700
249.437418	11748.372584	27.568717
249.575957	11768.634347	27.573735
249.663232	11802.213814	27.578752
250.192759	11810.222870	27.583770
250.601861	11841.485088	27.588788
250.863728	11861.885729	27.593805
251.291903	11871.120063	27.598823
251.211037	11906.988545	27.603840
252.034300	11919.802837	27.608858
252.145233	11944.527617	27.613876
252.520083	11939.543671	27.618893
252.876258	11970.203541	27.623911
252.593297	11983.470089	27.628928
253.381077	12001.829445	27.633946
253.395838	12021.360400	27.638964
253.659353	12026.335512	27.643981
253.824038	12044.834893	27.648999
253.706270	12070.342930	27.654016
254.219603	12086.299969	27.659034
254.430806	12106.660448	27.664052
254.674859	12111.422151	27.669069
254.880130	12134.862454	27.674087
255.203839	12156.912409	27.679104
255.746198	12168.182695	27.684122
255.954923	12186.232992	27.689140
256.113301	12217.645298	27.694157
256.856324	12227.828359	27.699175
256.599628	12250.475396	27.704192
256.975511	12266.140981	27.709210
257.237584	12270.913147	27.714228
257.380622	12293.152281	27.719245
257.505030	12303.695220	27.724263
257.552491	12330.533801	27.729280
258.569323	12339.163782	27.734298
258.633115	12365.054323	27.739316
258.762498	12382.273391	27.744333
259.188291	12396.425304	27.749351
259.427478	12413.681412	27.754368
259.681643	12427.887707	27.759386
259.855326	12441.866233	27.764404
260.314058	12450.671208	27.769421
260.400925	12470.186854	27.774439
260.466832	12485.368924	27.779456
260.976162	12503.431363	27.784474
261.211398	12520.289591	27.789492
261.002657	12537.342518	27.794509
261.388859	12553.677133	27.799527
261.555017	12589.600860	27.804544
261.987875	12595.774058	27.809562
262.105991	12617.931095	27.814580
262.646886	12628.898626	27.819597
262.767784	12638.377193	27.824615
262.855487	12661.101837	27.829632
263.413062	12679.699331	27.834650
263.402795	12698.825559	27.839668
263.445935	12718.480301	27.844685
264.046752	12710.531130	27.849703
264.343584	12740.272605	27.854720
264.522778	12759.643351	27.859738
264.804792	12777.980800	27.864756
264.941125	12807.674859	27.869773
265.535716	12810.764537	27.874791
265.408750	12835.184119	27.879808
265.408257	12855.791666	27.884826
266.092070	12888.833635	27.889844
266.289765	12911.638153	27.894861
266.976616	12920.438786	27.899879
266.968362	12938.271296	27.904896
267.221742	12952.408064	27.909914
267.628214	12978.937867	27.914932
267.417756	13002.892475	27.919949
267.988229	13013.630053	27.924967
268.090357	13042.450936	27.929984
268.290715	13062.822292	27.935002
268.697546	13081.785516	27.940020
268.478036	13113.384119	27.945037
269.020399	13133.498939	27.950055
269.508713	13155.814577	27.955072
269.923229	13174.797125	27.960090
270.657642	13189.495955	27.965108
270.818731	13215.868145	27.970125
271.272335	13207.892631	27.975143
271.223336	13234.436652	27.980160
272.058091	13235.740800	27.985178
272.233226	13247.380578	27.990196
272.597887	13275.630622	27.995213
273.089784	13262.508634	28.000231
273.065021	13267.823276	28.005248
273.511709	13281.515546	28.010266
273.797221	13292.180635	28.015284
273.806618	13302.914986	28.020301
274.453575	13320.461603	28.025319
274.093663	13339.104294	28.030336
274.261420	13339.566890	28.035354
274.571135	13357.325267	28.040372
274.374397	13380.282281	28.045389
274.998065	13400.697580	28.050407
274.728261	13438.212689	28.055424
275.064029	13452.752287	28.060442
275.548290	13482.355434	28.065460
275.699570	13507.784253	28.070477
276.109513	13526.853063	28.075495
276.365935	13561.635777	28.080512
276.675690	13577.742965	28.085530
277.054819	13602.294393	28.090548
276.924442	13630.913642	28.095565
277.639317	13645.715392	28.100583
277.637211	13667.170439	28.105600
278.136307	13695.548706	28.110618
278.432551	13715.361392	28.115636
278.438399	13735.945374	28.120653
278.976326	13758.839847	28.125671
278.953079	13780.222898	28.130688
279.591086	13811.681183	28.135706
279.822826	13830.683669	28.140724
279.920299	13840.857018	28.145741
280.117017	13862.293656	28.150759
280.445306	13883.390269	28.155776
280.735889	13905.717551	28.160794
281.175733	13925.019840	28.165812
281.483377	13946.893675	28.170829
281.816354	13965.045982	28.175847
281.894943	13986.741827	28.180864
282.020816	14016.335825	28.185882
282.476566	14030.072933	28.190900
282.619309	14057.426538	28.195917
282.968126	14082.407602	28.200935
283.358580	14103.880311	28.205952
283.875334	14120.544779	28.210970
284.183133	14132.450078	28.215988
284.221965	14160.240199	28.221005
284.714758	14181.748106	28.226023
284.754645	14202.189956	28.231040
285.124546	14224.302863	28.236058
285.482499	14236.407965	28.241076
285.546829	14273.162237	28.246093
285.856437	14289.358406	28.251111
286.531198	14303.503953	28.256128
286.485847	14328.350384	28.261146
286.984018	14343.637699	28.266164
286.898872	14368.881581	28.271181
287.138327	14383.559270	28.276199
287.536821	14409.635736	28.281216
287.928551	14442.929274	28.286234
288.500775	14453.837719	28.291252
288.573309	14479.123483	28.296269
288.761188	14506.621671	28.301287
289.104550	14532.061332	28.306304
289.064070	14552.720189	28.311322
289.498154	14578.069291	28.316340
290.135294	14620.328828	28.321357
289.874978	14636.406758	28.326375
290.518450	14666.997485	28.331392
290.477549	14687.655006	28.336410
291.166973	14703.892846	28.341428
291.230840	14741.193511	28.346445
291.938488	14762.728152	28.351463
292.247465	14789.322729	28.356480
292.385807	14809.303094	28.361498
292.827658	14827.849691	28.366516
292.644909	14851.625939	28.371533
293.300610	14871.691103	28.376551
293.889651	14905.547108	28.381568
293.737913	14910.605904	28.386586
294.258656	14945.557506	28.391604
294.423824	14960.835808	28.396621
294.412135	14996.173335	28.401639
294.923218	15013.178482	28.406656
294.899363	15042.830602	28.411674
295.663306	15074.773252	28.416692
295.601644	15100.849630	28.421709
295.916041	15121.798857	28.426727
296.263722	15158.450002	28.431744
296.137354	15187.203699	28.436762
296.901472	15206.431874	28.441780
297.178866	15241.120159	28.446797
297.599810	15260.056810	28.451815
298.273921	15288.998354	28.456832
298.317705	15307.853961	28.461850
299.241376	15313.137076	28.466868
299.546616	15342.700698	28.471885
299.318503	15356.607073	28.476903
299.992735	15378.507371	28.481920
299.866256	15384.263442	28.486938
300.232691	15401.138449	28.491956
300.708272	15425.318955	28.496973
300.623988	15449.407605	28.501991
301.236401	15466.103356	28.507008
301.031715	15490.196198	28.512026
301.533065	15512.076383	28.517044
301.498317	15537.466614	28.522061
301.735747	15556.682934	28.527079
302.168988	15579.847853	28.532096
302.001139	15613.778372	28.537114
302.743046	15638.427387	28.542132
303.032073	15666.369432	28.547149
303.415918	15698.568373	28.552167
303.641794	15715.807343	28.557184
303.636660	15757.827649	28.562202
304.360736	15777.236475	28.567220
304.479915	15817.482307	28.572237
304.550124	15839.115809	28.577255
305.221519	15872.695447	28.582272
305.622966	15899.958970	28.587290
306.405882	15913.776006	28.592308
306.543560	15934.782266	28.597325
306.999037	15952.390164	28.602343
307.647140	15971.915792	28.607360
307.650483	15998.376865	28.612378
308.004897	16003.300365	28.617396
307.863932	16029.079271	28.622413
308.628257	16048.076733	28.627431
308.791198	16065.473039	28.632448
308.955785	16091.239387	28.637466
309.387398	16113.226462	28.642484
309.549626	16140.810442	28.647501
309.528619	16170.298650	28.652519
309.933144	16188.441618	28.657536
310.414891	16227.605707	28.662554
311.013176	16247.392063	28.667572
311.327650	16267.472771	28.672589
311.276962	16293.367989	28.677607
311.476650	16318.673416	28.682624
311.919944	16339.585574	28.687642
312.330624	16372.214824	28.692660
312.819867	16392.203768	28.697677
312.643536	16419.483234	28.702695
313.266673	16445.079816	28.707712
313.482360	16476.819491	28.712730
314.161745	16497.870942	28.717748
314.422048	16514.410019	28.722765
314.795319	16537.912451	28.727783
314.896934	16553.343012	28.732800
315.356811	16577.102277	28.737818
315.897810	16596.167220	28.742836
315.982807	16618.087729	28.747853
316.266005	16655.058641	28.752871
316.859661	16659.525152	28.757888
316.771303	16694.089389	28.762906
317.388090	16710.159986	28.767924
317.601637	16720.708400	28.772941
317.897968	16760.150265	28.777959
318.537941	16764.902308	28.782976
318.446106	16799.780984	28.787994
318.843830	16818.357625	28.793012
318.909918	16849.279523	28.798029
318.829795	16878.874912	28.803047
319.505781	16901.596541	28.808064
319.545679	16933.700276	28.813082
320.258469	16957.375754	28.818100
320.481819	16985.187472	28.823117
320.607218	17009.481762	28.828135
320.836511	17024.295899	28.833152
321.241846	17056.591680	28.838170
321.867618	17076.169602	28.843188
321.918244	17101.924841	28.848205
322.335860	17130.953003	28.853223
322.805872	17150.731698	28.858240
323.181252	17178.575367	28.863258
323.326866	17207.550883	28.868276
323.704048	17224.998135	28.873293
323.857599	17260.959458	28.878311
324.322180	17276.510413	28.883328
324.400991	17310.049049	28.888346
324.648253	17340.621979	28.893364
324.772183	17368.583167	28.898381
324.772942	17407.430770	28.903399
325.656691	17428.692384	28.908416
325.698892	17474.564541	28.913434
326.346338	17498.874181	28.918452
326.596678	17527.183576	28.923469
326.667453	17569.544304	28.928487
327.340058	17595.202285	28.933504
327.425744	17637.656871	28.938522
327.790880	17666.659973	28.943540
328.324637	17687.175892	28.948557
328.090687	17724.247254	28.953575
329.118967	17755.175811	28.958592
328.618290	17787.217626	28.963610
329.326979	17819.724859	28.968628
330.160865	17862.253437	28.973645
329.888636	17899.323633	28.978663
330.261153	17929.933707	28.983680
330.395720	17969.586457	28.988698
331.220399	18013.612770	28.993716
331.779142	18042.620800	28.998733
332.342127	18076.229167	29.003751
332.542167	18105.195691	29.008768
332.945079	18131.304153	29.013786
333.554515	18149.019803	29.018804
334.070080	18176.038122	29.023821
333.764046	18208.720069	29.028839
334.416420	18230.884724	29.033856
334.897836	18265.071243	29.038874
335.077784	18280.708002	29.043892
335.466436	18310.696654	29.048909
335.844730	18341.520905	29.053927
336.133555	18361.074061	29.058944
336.189264	18389.202720	29.063962
336.566549	18421.718603	29.068980
337.169011	18447.785141	29.073997
337.210502	18476.047126	29.079015
337.617972	18500.859736	29.084032
338.063354	18523.990552	29.089050
338.245514	18544.269288	29.094068
339.092237	18565.182256	29.099085
339.331995	18597.574614	29.104103
339.836644	18623.266674	29.109120
339.771959	18647.832796	29.114138
340.006259	18687.377790	29.119156
340.778729	18698.738341	29.124173
340.899885	18730.764365	29.129191
341.270491	18754.404386	29.134208
341.115794	18784.972312	29.139226
341.897046	18815.310006	29.144244
342.177504	18838.928786	29.149261
342.359255	18857.757785	29.154279
342.613201	18878.248906	29.159296
343.329833	18909.678788	29.164314
343.532962	18941.018595	29.169332
344.409404	18958.167672	29.174349
344.070852	18977.136359	29.179367
344.633783	18998.270156	29.184384
344.576670	19020.149550	29.189402
344.984809	19042.377714	29.194420
345.595076	19075.680803	29.199437
345.217008	19100.034547	29.204455
345.819744	19128.291618	29.209472
346.143423	19159.135873	29.214490
346.503239	19193.230905	29.219508
347.088377	19230.263317	29.224525
347.229361	19263.893374	29.229543
347.720081	19292.670506	29.234560
348.102708	19316.495351	29.239578
348.066463	19356.767614	29.244596
348.259879	19383.179065	29.249613
348.433532	19424.835526	29.254631
349.650136	19455.360992	29.259648
349.772946	19483.614411	29.264666
349.983821	19524.799948	29.269684
350.410697	19553.493499	29.274701
350.735710	19582.013188	29.279719
351.394778	19612.993618	29.284736
351.650722	19635.112153	29.289754
351.982786	19675.161973	29.294772
352.785562	19694.379576	29.299789
352.869572	19726.137790	29.304807
353.324830	19754.344628	29.309824
353.857525	19784.906446	29.314842
353.951109	19820.377216	29.319860
354.329747	19834.289577	29.324877
354.074886	19876.467232	29.329895
354.578813	19906.040900	29.334912
354.937246	19937.785709	29.339930
355.342208	19979.728507	29.344948
355.964684	20011.532301	29.349965
356.197324	20044.043734	29.354983
356.098004	20077.295809	29.360000
356.614372	20106.883543	29.365018
356.954539	20143.941121	29.370036
357.221423	20180.178539	29.375053
357.413295	20227.482311	29.380071
358.017373	20260.807718	29.385088
358.454460	20300.110228	29.390106
358.890409	20349.607826	29.395124
359.113733	20370.194125	29.400141
359.077542	20416.295453	29.405159
359.592861	20452.601194	29.410176
360.216194	20497.353126	29.415194
360.543325	20540.112604	29.420212
361.148716	20575.781034	29.425229
361.518693	20618.022862	29.430247
361.854764	20647.239344	29.435264
362.613923	20676.849462	29.440282
362.881696	20709.517186	29.445300
363.406274	20726.540207	29.450317
363.725565	20759.134882	29.455335
363.986235	20797.294812	29.460352
364.167749	20824.032113	29.465370
364.880292	20871.713601	29.470388
365.234935	20889.581481	29.475405
365.178248	20922.473484	29.480423
365.625444	20957.355396	29.485440
366.219425	20987.329147	29.490458
366.245530	21031.728722	29.495476
366.510734	21058.391089	29.500493
366.872541	21097.529769	29.505511
367.366518	21116.992369	29.510528
367.913347	21161.528550	29.515546
368.053297	21205.704831	29.520564
368.672446	21211.301903	29.525581
369.195313	21247.565561	29.530599
369.318386	21272.569602	29.535616
369.776420	21290.250567	29.540634
370.148554	21321.105007	29.545652
370.581694	21352.535895	29.550669
370.924467	21386.330806	29.555687
371.238481	21406.170312	29.560704
371.485896	21440.461928	29.565722
371.794958	21462.372313	29.570740
372.220541	21495.192074	29.575757
372.318514	21533.140924	29.580775
372.339806	21574.766433	29.585792
373.017377	21619.078857	29.590810
373.249405	21649.361110	29.595828
373.573887	21687.547211	29.600845
374.129931	21726.144465	29.605863
374.346919	21769.628428	29.610880
374.745747	21804.961536	29.615898
374.717941	21840.754614	29.620916
375.225436	21894.746087	29.625933
375.519117	21935.178161	29.630951
375.677605	21986.757079	29.635968
376.202037	22029.155103	29.640986
376.966708	22084.556744	29.646004
377.778047	22117.358138	29.651021
378.356835	22164.348049	29.656039
378.584596	22209.259775	29.661056
378.981559	22227.457911	29.666074
379.246844	22271.770798	29.671092
379.601520	22309.934406	29.676109
380.350805	22336.093146	29.681127
380.609839	22369.743055	29.686144
380.997545	22401.974881	29.691162
381.291376	22440.758992	29.696180
381.924442	22470.415192	29.701197
382.637729	22504.466471	29.706215
382.717120	22532.863070	29.711232
383.546203	22555.125703	29.716250
383.486305	22590.957210	29.721268
384.135395	22616.804998	29.726285
384.287529	22650.697012	29.731303
384.157075	22692.265213	29.736320
384.564453	22718.518872	29.741338
385.033693	22764.355524	29.746356
385.005625	22802.143588	29.751373
385.825554	22842.448335	29.756391
385.648324	22891.758320	29.761408
386.241573	22927.909920	29.766426
386.605240	22979.804851	29.771444
387.070559	23015.131093	29.776461
387.439967	23057.052779	29.781479
387.482029	23105.412680	29.786496
388.407729	23136.992579	29.791514
388.740617	23190.460479	29.796532
389.240461	23222.870861	29.801549
389.681108	23264.104886	29.806567
389.908097	23305.416879	29.811584
390.513854	23343.099867	29.816602
390.989040	23380.914881	29.821620
391.462086	23415.420791	29.826637
391.909547	23458.167818	29.831655
392.553857	23475.167548	29.836672
392.523613	23513.055317	29.841690
393.026316	23553.619146	29.846708
393.008468	23575.761308	29.851725
393.634388	23622.548830	29.856743
394.072232	23662.934427	29.861760
394.338004	23682.415629	29.866778
394.638232	23716.821410	29.871796
394.895082	23758.132729	29.876813
395.281734	23803.044521	29.881831
395.284012	23833.371805	29.886848
396.138205	23872.670534	29.891866
396.190544	23921.609741	29.896884
396.265998	23963.656343	29.901901
396.529461	24017.329113	29.906919
397.132882	24069.777495	29.911936
397.669247	24107.631330	29.916954
397.880727	24163.670448	29.921972
398.262024	24215.108984	29.926989
398.733739	24256.141617	29.932007
399.202782	24308.735928	29.937024
399.942999	24343.019837	29.942042
400.151547	24396.953592	29.947060
400.823251	24436.591256	29.952077
401.098138	24471.849507	29.957095
401.649615	24527.106742	29.962112
402.405560	24562.990554	29.967130
403.181663	24597.429887	29.972148
403.361154	24639.453090	29.977165
403.936531	24675.291281	29.982183
404.389145	24710.285718	29.987200
404.745862	24737.772936	29.992218
405.103541	24789.698052	29.997236
405.336693	24820.909839	30.002253
405.862648	24852.040200	30.007271
405.765434	24895.972015	30.012288
406.238023	24932.836920	30.017306
406.792898	24977.537959	30.022324
407.240573	25008.039752	30.027341
407.802240	25053.804257	30.032359
408.156697	25085.526320	30.037376
408.924431	25116.223004	30.042394
409.122058	25157.312553	30.047412
409.625261	25182.015166	30.052429
410.264238	25215.194819	30.057447
410.178768	25266.425074	30.062464
410.897422	25288.859367	30.067482
411.144624	25330.926706	30.072500
411.443553	25378.698729	30.077517
411.945596	25409.964944	30.082535
412.144111	25451.152823	30.087552
412.737086	25490.108956	30.092570
412.973173	25526.482796	30.097588
413.352957	25579.792780	30.102605
413.904842	25609.400089	30.107623
414.027330	25656.448266	30.112640
414.591675	25686.362728	30.117658
414.891054	25735.542301	30.122676
415.157210	25790.461266	30.127693
415.785488	25830.774825	30.132711
415.972494	25875.661992	30.137728
416.530518	25914.684792	30.142746
417.074347	25967.385413	30.147764
417.690700	26004.358198	30.152781
418.419652	26039.855346	30.157799
418.350679	26086.387550	30.162816
419.069062	26117.600400	30.167834
419.283220	26162.117976	30.172852
419.595478	26209.861735	30.177869
420.026746	26244.496989	30.182887
420.227323	26288.332724	30.187904
420.789242	26327.551371	30.192922
421.185079	26376.549690	30.197940
421.439690	26416.528955	30.202957
421.837885	26450.447823	30.207975
422.189031	26505.938535	30.212992
422.587042	26543.815911	30.218010
423.138995	26587.118107	30.223028
423.335799	26628.044162	30.228045
423.513455	26681.359428	30.233063
423.756800	26733.298300	30.238080
424.512023	26775.072368	30.243098
425.048294	26813.211365	30.248116
425.441138	26871.557117	30.253133
425.921622	26906.781701	30.258151
426.099989	26969.894355	30.263168
426.913215	27015.882773	30.268186
427.043791	27067.800281	30.273204
427.115818	27127.218679	30.278221
427.785443	27165.544602	30.283239
428.058760	27230.273216	30.288256
428.255177	27278.830777	30.293274
428.995694	27333.329363	30.298292
429.875987	27387.391835	30.303309
430.484906	27423.873706	30.308327
430.640101	27475.744220	30.313344
431.217951	27522.536192	30.318362
431.394958	27569.814019	30.323380
432.085635	27616.559221	30.328397
432.666934	27667.725924	30.333415
432.984192	27714.331208	30.338432
433.627217	27757.189179	30.343450
434.180513	27803.471829	30.348468
434.417718	27854.348961	30.353485
435.420967	27894.501340	30.358503
435.734228	27941.417016	30.363520
435.945463	27972.174486	30.368538
436.685056	28011.500110	30.373556
436.650238	28069.586214	30.378573
437.263647	28106.658646	30.383591
437.637514	28155.277682	30.388608
437.835958	28201.424452	30.393626
438.206560	28249.236785	30.398644
438.461271	28296.301888	30.403661
439.219121	28340.918239	30.408679
439.548608	28403.869232	30.413696
440.321423	28450.120509	30.418714
440.838343	28489.203267	30.423732
440.843063	28544.297235	30.428749
441.591928	28589.754781	30.433767
441.780721	28641.897679	30.438784
442.074098	28685.225789	30.443802
442.897526	28724.356232	30.448820
443.084650	28786.385807	30.453837
443.308012	28821.808194	30.458855
443.896108	28889.121832	30.463872
444.201738	28934.196107	30.468890
444.899180	28981.167856	30.473908
445.354326	29038.087978	30.478925
445.937986	29083.034696	30.483943
445.907800	29142.256091	30.488960
446.149451	29194.581189	30.493978
447.245728	29240.506706	30.498996
447.850478	29301.794068	30.504013
448.257164	29342.297572	30.509031
448.712727	29388.048567	30.514048
448.925336	29434.978608	30.519066
449.422188	29483.887051	30.524084
449.755051	29542.876339	30.529101
450.262933	29579.871570	30.534119
450.720858	29628.767923	30.539136
450.766748	29678.246678	30.544154
451.602329	29717.579254	30.549172
452.078284	29771.141844	30.554189
452.540392	29815.306112	30.559207
453.285674	29869.635252	30.564224
453.200649	29925.606485	30.569242
453.644570	29961.357547	30.574260
454.219611	30006.781279	30.579277
454.589562	30052.283172	30.584295
454.814332	30106.064947	30.589312
455.148828	30160.999150	30.594330
455.792826	30211.636182	30.599348
456.114770	30275.040016	30.604365
456.439993	30325.001299	30.609383
456.993422	30377.123869	30.614400
457.484351	30431.367436	30.619418
458.222582	30483.144324	30.624436
458.676236	30549.420296	30.629453
458.973994	30605.349405	30.634471
459.779923	30654.178532	30.639488
460.042238	30697.295952	30.644506
460.596278	30758.104674	30.649524
461.217425	30801.825584	30.654541
461.795719	30853.074745	30.659559
461.992587	30899.421380	30.664576
462.485773	30961.143139	30.669594
463.040489	31016.624144	30.674612
463.478203	31066.619444	30.679629
463.867232	31116.509354	30.684647
464.421226	31169.574345	30.689664
464.802807	31231.713007	30.694682
465.686743	31269.369018	30.699700
465.790280	31331.771652	30.704717
466.281935	31383.519378	30.709735
466.978369	31427.693188	30.714752
467.334429	31485.975356	30.719770
467.661956	31538.719213	30.724788
468.169164	31595.853622	30.729805
468.563835	31647.447782	30.734823
469.114310	31701.552945	30.739840
469.493994	31760.027728	30.744858
470.128213	31804.304259	30.749876
470.625645	31864.908483	30.754893
471.018379	31905.855631	30.759911
471.853708	31959.804112	30.764928
472.435984	32017.394435	30.769946
472.826466	32057.282223	30.774964
473.239685	32117.090386	30.779981
473.731463	32155.895263	30.784999
474.207262	32216.355986	30.790016
474.375897	32268.885344	30.795034
475.483729	32319.988223	30.800052
475.448148	32383.386178	30.805069
475.660993	32422.505901	30.810087
476.822718	32468.722541	30.815104
476.904300	32519.149954	30.820122
477.363414	32563.327965	30.825140
477.752244	32634.203755	30.830157
478.097621	32666.654273	30.835175
478.558621	32719.013629	30.840192
479.067597	32781.840327	30.845210
479.638626	32841.640659	30.850228
479.637740	32905.242999	30.855245
480.087991	32954.547464	30.860263
480.831925	33024.072535	30.865280
480.978835	33080.107013	30.870298
481.868332	33137.300024	30.875316
481.933042	33198.904797	30.880333
482.401424	33250.652397	30.885351
482.843468	33299.769866	30.890368
483.469099	33349.784792	30.895386
483.770991	33405.763149	30.900404
484.598279	33467.362792	30.905421
484.916542	33534.682078	30.910439
486.057947	33582.684584	30.915456
485.724067	33645.158197	30.920474
486.604219	33700.877892	30.925492
486.882589	33759.082596	30.930509
487.474535	33808.984483	30.935527
488.020796	33863.661787	30.940544
487.996267	33926.148396	30.945562
488.647005	33983.891599	30.950580
489.044174	34044.895363	30.955597
489.574163	34107.123777	30.960615
490.436760	34170.764729	30.965632
490.736061	34233.410340	30.970650
491.530808	34284.397083	30.975668
492.014887	34348.549268	30.980685
492.701516	34398.317268	30.985703
493.287078	34463.043172	30.990720
493.546884	34521.726763	30.995738
493.957118	34573.191217	31.000756
494.432867	34621.189744	31.005773
494.850670	34690.617458	31.010791
495.498413	34748.783326	31.015808
495.963009	34806.010893	31.020826
496.744526	34863.650157	31.025844
496.807049	34927.463847	31.030861
497.564114	34993.050057	31.035879
497.959685	35053.312837	31.040896
498.055837	35116.553648	31.045914
499.273391	35167.514109	31.050932
499.502415	35235.110180	31.055949
499.825278	35292.151297	31.060967
500.623048	35337.829689	31.065984
500.763775	35410.783458	31.071002
501.623919	35473.918271	31.076020
502.189520	35547.029621	31.081037
502.423531	35599.718984	31.086055
503.287020	35653.800309	31.091072
503.483817	35728.172472	31.096090
504.022689	35787.893375	31.101108
504.477649	35845.526643	31.106125
505.062363	35912.725709	31.111143
505.797312	35958.463403	31.116160
505.883289	36032.971900	31.121178
506.882848	36084.681034	31.126196
507.456756	36146.514850	31.131213
507.571548	36196.240321	31.136231
508.210169	36256.154591	31.141248
508.888435	36343.012907	31.146266
509.396371	36387.738321	31.151284
510.104903	36452.258627	31.156301
510.325526	36506.060556	31.161319
510.999582	36561.245739	31.166336
511.544597	36610.099714	31.171354
511.903840	36666.123023	31.176372
512.633964	36729.135422	31.181389
513.111093	36786.168442	31.186407
513.768522	36836.973726	31.191424
513.869059	36902.867898	31.196442
514.268375	36964.241055	31.201460
515.148046	37029.732432	31.206477
515.397377	37091.231786	31.211495
515.974263	37150.202996	31.216512
516.139991	37205.938049	31.221530
516.362664	37260.966402	31.226548
516.880394	37320.320344	31.231565
517.399746	37377.859532	31.236583
517.973763	37432.391695	31.241600
518.293729	37506.520493	31.246618
518.829829	37569.722531	31.251636
519.717126	37635.375810	31.256653
519.705392	37708.711261	31.261671
520.440379	37762.334147	31.266688
520.860874	37843.151143	31.271706
521.174255	37899.914915	31.276724
522.007850	37971.615831	31.281741
522.482028	38044.042334	31.286759
523.283419	38102.004347	31.291776
523.154493	38180.470786	31.296794
524.020764	38246.347534	31.301812
524.512438	38321.546488	31.306829
524.980920	38390.459389	31.311847
525.599937	38473.948072	31.316864
526.371076	38530.742366	31.321882
527.168859	38603.000877	31.326900
527.313021	38672.877404	31.331917
527.790593	38743.544990	31.336935
528.362869	38812.931565	31.341952
528.465855	38893.370138	31.346970
529.347286	38975.034515	31.351988
530.228274	39031.622861	31.357005
530.326478	39105.233025	31.362023
531.358855	39170.160912	31.367040
531.594503	39240.759926	31.372058
532.262227	39306.960552	31.377076
533.089405	39374.078819	31.382093
533.849857	39444.083770	31.387111
534.767412	39503.214705	31.392128
534.923428	39558.182143	31.397146
535.201390	39627.386876	31.402164
536.221567	39696.450336	31.407181
536.348025	39755.094112	31.412199
537.097508	39822.226868	31.417216
537.314713	39893.109221	31.422234
537.818601	39952.748686	31.427252
538.627576	40032.296047	31.432269
539.101031	40097.259596	31.437287
539.438995	40173.466947	31.442304
539.667615	40242.578001	31.447322
540.350619	40316.235348	31.452340
540.786550	40385.751452	31.457357
541.055371	40472.662508	31.462375
541.922081	40536.587304	31.467392
542.920746	40603.757535	31.472410
543.051660	40665.578966	31.477428
543.959956	40736.741853	31.482445
544.012765	40812.920056	31.487463
544.699041	40879.410577	31.492480
545.013834	40961.950820	31.497498
545.543767	41038.000644	31.502516
546.468338	41110.443877	31.507533
546.873514	41195.549198	31.512551
547.393437	41271.737381	31.517568
547.794349	41343.949211	31.522586
548.468515	41411.696857	31.527604
548.695656	41491.870678	31.532621
549.261507	41574.953040	31.537639
549.723582	41651.452240	31.542656
550.587281	41723.213473	31.547674
550.873853	41814.136990	31.552692
551.939025	41892.617868	31.557709
551.761272	41963.450354	31.562727
552.696294	42024.916257	31.567744
553.213203	42090.024907	31.572762
553.628903	42166.252954	31.577780
554.561719	42235.078419	31.582797
555.317266	42316.036675	31.587815
555.493057	42390.196517	31.592832
556.130158	42440.720924	31.597850
556.623591	42532.936538	31.602868
557.324978	42599.017239	31.607885
557.870499	42667.835685	31.612903
558.135731	42735.917773	31.617920
558.933194	42809.073743	31.622938
559.547259	42884.441727	31.627956
560.057015	42949.863972	31.632973
560.622478	43035.680572	31.637991
560.872163	43104.287481	31.643008
561.597521	43187.518084	31.648026
562.095723	43256.217100	31.653044
562.969589	43321.959358	31.658061
563.597634	43407.530572	31.663079
564.189906	43480.107473	31.668096
564.519296	43552.437632	31.673114
565.238264	43623.295683	31.678132
565.838447	43698.296743	31.683149
566.381691	43786.772422	31.688167
566.740813	43852.942551	31.693184
567.365743	43932.537185	31.698202
567.751126	44014.602702	31.703220
568.508274	44086.996889	31.708237
569.228253	44155.552106	31.713255
569.721271	44235.984370	31.718272
570.495399	44311.786350	31.723290
570.829960	44410.705476	31.728308
571.413224	44472.174477	31.733325
572.012525	44562.630461	31.738343
572.816368	44637.109147	31.743360
573.392722	44704.578770	31.748378
573.945454	44789.761506	31.753396
574.831472	44854.954671	31.758413
575.198983	44930.368528	31.763431
575.756768	45011.904802	31.768448
576.154130	45084.974808	31.773466
576.531791	45172.376211	31.778484
577.219737	45244.881050	31.783501
578.240737	45332.322178	31.788519
578.303357	45409.348050	31.793536
579.074131	45474.458221	31.798554
579.285795	45559.119846	31.803572
580.001866	45639.754964	31.808589
580.188402	45739.769616	31.813607
581.293618	45808.611438	31.818624
582.091712	45906.757819	31.823642
582.475021	45982.744804	31.828660
583.008647	46054.684669	31.833677
583.544353	46139.317493	31.838695
584.088773	46221.470634	31.843712
585.066626	46297.865892	31.848730
585.460335	46380.350899	31.853748
586.328273	46460.077201	31.858765
586.603753	46541.038411	31.863783
587.162266	46625.540199	31.868800
587.852375	46704.122299	31.873818
588.566998	46790.212559	31.878836
588.882488	46858.086675	31.883853
589.392205	46946.604948	31.888871
589.883853	47028.896636	31.893888
590.750349	47104.925180	31.898906
590.931433	47186.823626	31.903924
591.574251	47261.393021	31.908941
592.124062	47341.503997	31.913959
592.924859	47416.439463	31.918976
593.609732	47495.635162	31.923994
594.041146	47569.034449	31.929012
594.916184	47633.437028	31.934029
595.752993	47705.680475	31.939047
596.506955	47780.713540	31.944064
597.220082	47855.210513	31.949082
597.482473	47930.912707	31.954100
597.958274	47989.887923	31.959117
598.451837	48072.041738	31.964135
599.184297	48154.229082	31.969152
599.837918	48221.445949	31.974170
600.113707	48306.301947	31.979188
600.567601	48388.239479	31.984205
601.454605	48466.894286	31.989223
601.641911	48565.954326	31.994240
602.550061	48634.504294	31.999258
603.034314	48731.908789	32.004276
603.236275	48806.847614	32.009293
604.108155	48898.839433	32.014311
604.533689	48985.356908	32.019328
605.139661	49065.431159	32.024346
605.903153	49159.223228	32.029364
606.366958	49245.536612	32.034381
607.086581	49343.871708	32.039399
607.608093	49436.220846	32.044416
608.290697	49527.277452	32.049434
609.055346	49617.900921	32.054452
609.524227	49705.822996	32.059469
610.241328	49791.196964	32.064487
610.676042	49888.160787	32.069504
611.223178	49993.399733	32.074522
611.668366	50082.180143	32.079540
612.322926	50173.664492	32.084557
613.350376	50274.896929	32.089575
613.630872	50354.904018	32.094592
614.864611	50442.561035	32.099610
615.516200	50528.324938	32.104628
615.912308	50628.109681	32.109645
616.446189	50706.247780	32.114663
617.354053	50801.612654	32.119680
618.288414	50893.332152	32.124698
618.426528	50972.853696	32.129716
618.961853	51071.705010	32.134733
619.339299	51151.604658	32.139751
620.367763	51259.376653	32.144768
621.128653	51346.026276	32.149786
621.529521	51435.581423	32.154804
621.949624	51527.366774	32.159821
622.793519	51621.110246	32.164839
623.195334	51714.680835	32.169856
624.124049	51798.844387	32.174874
624.069831	51904.253131	32.179892
625.146523	51992.300060	32.184909
625.786143	52084.263419	32.189927
626.569946	52186.657942	32.194944
627.677671	52263.725298	32.199962
628.201083	52349.467948	32.204980
629.039480	52429.347293	32.209997
629.916883	52505.834587	32.215015
630.570997	52600.678583	32.220032
631.024036	52662.448309	32.225050
631.781802	52750.232354	32.230068
632.313823	52830.795670	32.235085
632.879536	52900.810386	32.240103
633.305588	52990.033764	32.245120
633.796545	53047.509073	32.250138
634.318899	53139.048286	32.255156
634.690023	53224.586221	32.260173
635.159554	53301.725211	32.265191
635.815467	53385.075249	32.270208
636.484171	53470.337693	32.275226
637.061426	53574.750995	32.280244
637.203204	53656.759380	32.285261
637.797956	53759.477714	32.290279
638.613691	53847.522476	32.295296
639.365880	53939.172796	32.300314
640.285423	54036.582778	32.305332
640.987787	54128.823433	32.310349
641.266294	54211.929781	32.315367
641.675991	54315.408129	32.320384
642.672916	54420.773788	32.325402
643.378208	54511.316313	32.330420
643.732541	54604.564350	32.335437
644.613315	54693.202370	32.340455
645.393808	54796.280864	32.345472
645.886963	54889.703182	32.350490
646.448264	54991.934412	32.355508
647.004125	55104.812715	32.360525
648.169477	55196.122704	32.365543
647.848034	55306.215544	32.370560
648.730416	55395.816806	32.375578
649.526295	55517.237661	32.380596
650.129422	55611.346552	32.385613
651.150571	55713.391866	32.390631
651.715491	55818.015034	32.395648
652.578273	55929.021444	32.400666
653.052523	56034.798006	32.405684
653.845510	56129.099152	32.410701
654.712462	56220.039863	32.415719
655.037734	56332.710564	32.420736
655.687733	56426.594469	32.425754
656.142974	56529.811589	32.430772
656.813054	56639.703886	32.435789
657.873212	56745.949828	32.440807
658.324621	56855.784665	32.445824
659.083905	56949.804649	32.450842
659.717837	57053.171906	32.455860
660.616390	57148.793692	32.460877
661.460223	57246.484833	32.465895
662.370538	57354.079371	32.470912
663.047601	57439.667281	32.475930
663.522905	57533.654795	32.480948
663.941233	57632.321680	32.485965
664.955920	57728.609501	32.490983
665.294533	57832.471903	32.496000
665.988962	57927.789943	32.501018
666.872322	58024.075611	32.506036
667.344767	58123.854429	32.511053
667.993311	58226.751467	32.516071
668.807552	58324.673958	32.521088
669.443006	58433.804681	32.526106
670.002768	58532.743341	32.531124
670.486389	58629.053719	32.536141
671.067719	58742.871141	32.541159
671.587379	58845.584128	32.546176
672.198195	58947.713867	32.551194
672.994475	59048.549669	32.556212
673.793262	59152.797921	32.561229
674.418312	59260.753191	32.566247
674.970783	59380.696006	32.571264
675.620484	59490.537899	32.576282
676.180612	59586.878167	32.581300
676.786303	59692.639838	32.586317
677.643860	59798.177207	32.591335
677.863369	59891.535568	32.596352
678.383140	60012.530261	32.601370
679.247820	60120.899263	32.606388
679.552585	60235.112082	32.611405
680.571912	60339.102571	32.616423
680.559430	60454.613979	32.621440
681.750150	60564.719968	32.626458
682.699453	60675.877574	32.631476
683.227969	60794.537246	32.636493
684.135098	60897.556955	32.641511
684.737795	61014.632057	32.646528
685.297201	61129.092270	32.651546
686.305930	61237.670997	32.656564
686.823723	61354.344978	32.661581
687.953480	61450.732797	32.666599
688.334836	61583.432622	32.671616
689.276426	61682.001398	32.676634
690.061460	61773.916268	32.681652
690.747662	61896.929801	32.686669
692.127190	61988.974986	32.691687
692.743816	62097.326034	32.696704
693.539080	62188.659645	32.701722
694.385738	62286.197893	32.706740
694.758610	62390.628021	32.711757
695.723596	62491.598538	32.716775
696.162414	62599.880504	32.721792
696.665838	62691.782831	32.726810
697.030599	62804.028290	32.731828
697.460400	62912.047948	32.736845
698.517172	63024.180333	32.741863
698.842638	63145.048845	32.746880
699.420275	63262.077829	32.751898
700.343499	63378.810229	32.756916
700.979105	63494.168676	32.761933
701.732763	63603.130825	32.766951
702.188274	63718.817346	32.771968
703.278707	63837.168103	32.776986
704.251886	63956.076165	32.782004
704.880777	64067.861449	32.787021
705.841946	64169.270693	32.792039
706.415556	64290.041769	32.797056
707.000779	64397.063869	32.802074
707.650052	64513.538252	32.807092
708.298906	64617.200940	32.812109
709.601048	64728.088518	32.817127
710.232688	64849.516989	32.822144
710.886103	64951.891134	32.827162
711.577983	65056.844730	32.832180
711.989632	65181.225471	32.837197
712.798890	65280.819533	32.842215
713.966726	65396.675974	32.847232
714.251498	65509.436149	32.852250
714.865490	65620.322068	32.857268
715.637671	65732.396130	32.862285
716.862656	65839.851040	32.867303
717.209950	65952.059672	32.872320
717.698547	66062.216431	32.877338
718.410071	66177.653218	32.882356
719.197897	66295.360067	32.887373
720.141928	66407.820290	32.892391
720.606649	66517.812730	32.897408
721.325962	66633.162260	32.902426
722.289358	66746.891739	32.907444
722.319655	66871.604776	32.912461
723.173460	66974.259251	32.917479
723.752161	67099.755465	32.922496
724.654746	67215.798621	32.927514
725.536795	67314.758253	32.932532
726.168106	67425.581400	32.937549
726.441534	67529.466043	32.942567
727.182876	67644.476154	32.947584
727.712047	67777.615031	32.952602
728.675181	67885.559954	32.957620
729.144893	68013.178510	32.962637
729.870076	68123.863414	32.967655
730.436786	68253.635841	32.972672
731.242989	68382.838469	32.977690
732.120025	68506.751275	32.982708
732.919514	68636.689933	32.987725
733.387820	68757.814130	32.992743
734.327065	68887.914600	32.997760
734.941248	69016.741893	33.002778
735.827407	69139.518920	33.007796
736.601750	69285.966811	33.012813
737.218951	69400.305258	33.017831
738.057312	69534.497957	33.022848
738.747232	69652.549635	33.027866
739.847709	69780.915615	33.032884
740.679147	69903.035940	33.037901
741.335796	70030.351327	33.042919
742.169008	70163.252749	33.047936
743.168622	70279.657174	33.052954
743.923762	70416.176950	33.057972
744.027307	70543.498241	33.062989
745.541081	70652.637253	33.068007
746.728669	70769.228292	33.073024
747.200888	70889.459891	33.078042
748.341737	70989.108514	33.083060
748.873942	71121.458650	33.088077
749.343635	71237.039018	33.093095
750.428396	71352.012606	33.098112
751.127619	71484.571361	33.103130
751.661546	71587.256856	33.108148
752.533798	71720.686364	33.113165
752.871022	71850.057136	33.118183
753.568271	71969.125826	33.123200
754.507273	72107.801213	33.128218
755.097854	72231.833667	33.133236
755.641072	72369.804682	33.138253
756.409839	72494.428903	33.143271
757.121726	72619.537486	33.148288
757.476607	72745.243235	33.153306
758.528089	72896.153411	33.158324
759.041537	73024.465124	33.163341
759.443834	73170.286592	33.168359
760.923961	73308.051992	33.173376
761.827521	73442.669521	33.178394
762.630005	73574.888980	33.183412
763.401350	73705.596727	33.188429
763.449635	73836.418345	33.193447
764.329816	73984.695849	33.198464
765.366501	74120.775357	33.203482
766.456735	74239.330069	33.208500
767.150254	74383.695106	33.213517
767.866856	74520.165142	33.218535
769.071236	74659.805957	33.223552
769.539673	74785.245533	33.228570
770.483855	74915.268020	33.233588
771.022154	75045.725103	33.238605
771.728975	75183.427770	33.243623
772.751168	75320.396228	33.248640
773.271426	75451.446856	33.253658
774.361432	75585.174160	33.258676
774.868149	75710.638035	33.263693
775.223911	75836.203449	33.268711
776.159402	75968.877176	33.273728
776.705370	76102.488785	33.278746
777.669254	76231.889757	33.283764
778.595004	76361.082762	33.288781
779.023349	76488.037611	33.293799
780.088402	76615.899960	33.298816
780.963114	76753.793492	33.303834
781.468053	76884.709760	33.308852
782.191649	77025.754265	33.313869
782.941023	77159.629644	33.318887
784.095406	77278.278805	33.323904
784.890887	77418.573972	33.328922
786.210625	77545.944293	33.333940
787.080211	77679.562639	33.338957
787.406736	77813.587711	33.343975
788.199121	77943.861942	33.348992
788.942813	78080.786086	33.354010
789.950511	78216.345576	33.359028
790.282905	78338.285970	33.364045
791.005272	78494.399730	33.369063
792.098496	78619.283645	33.374080
792.439588	78770.674271	33.379098
793.169340	78908.244653	33.384116
794.088234	79051.660706	33.389133
794.611248	79199.969168	33.394151
795.742361	79343.756868	33.399168
796.585400	79493.171949	33.404186
797.168908	79620.340519	33.409204
798.263387	79772.556008	33.414221
799.171456	79912.873641	33.419239
800.231271	80051.294772	33.424256
800.888119	80201.162809	33.429274
801.816472	80335.287112	33.434292
802.689400	80472.318467	33.439309
803.367299	80629.725937	33.444327
804.233233	80757.980280	33.449344
804.750257	80907.091742	33.454362
805.737857	81042.342777	33.459380
806.523055	81203.209350	33.464397
807.366079	81330.629416	33.469415
808.420782	81476.246260	33.474432
808.792320	81626.442915	33.479450
809.660634	81767.645335	33.484468
810.794138	81910.550805	33.489485
811.596367	82060.078255	33.494503
812.460548	82201.638320	33.499520
813.091940	82345.774463	33.504538
814.507951	82472.359869	33.509556
815.762118	82598.036439	33.514573
816.418796	82734.010158	33.519591
817.377427	82870.966001	33.524608
818.310519	83006.883055	33.529626
818.901149	83133.975367	33.534644
819.767404	83274.542222	33.539661
820.108255	83413.431647	33.544679
820.960976	83533.169631	33.549696
821.529841	83685.884196	33.554714
822.352878	83820.963878	33.559732
823.001723	83966.448603	33.564749
823.612292	84108.714030	33.569767
824.750173	84258.611710	33.574784
825.515709	84399.429868	33.579802
826.556614	84553.970262	33.584820
827.099436	84688.164976	33.589837
827.608961	84829.382339	33.594855
828.651073	84979.553609	33.599872
829.228119	85135.307000	33.604890
829.742137	85265.081047	33.609908
830.771105	85413.555387	33.614925
831.634026	85564.892575	33.619943
832.615720	85697.508552	33.624960
833.576492	85843.402850	33.629978
834.336297	85976.949180	33.634996
834.762691	86132.936636	33.640013
835.511599	86269.700623	33.645031
836.547799	86422.666189	33.650048
837.467187	86573.443849	33.655066
838.467951	86719.697707	33.660084
839.671071	86847.696430	33.665101
840.581961	86991.505517	33.670119
841.433055	87122.866754	33.675136
842.982375	87269.697862	33.680154
843.909194	87386.678521	33.685172
845.082068	87510.079495	33.690189
845.504990	87651.024616	33.695207
846.482119	87775.629907	33.700224
847.377864	87907.829751	33.705242
847.922313	88046.896876	33.710260
849.035803	88172.405595	33.715277
849.633235	88312.870288	33.720295
850.419238	88446.521351	33.725312
851.294070	88584.398112	33.730330
851.674110	88720.300846	33.735348
852.647215	88865.490631	33.740365
853.361201	89012.590825	33.745383
854.283168	89160.745996	33.750400
855.046191	89317.312901	33.755418
855.519243	89455.925539	33.760436
856.194280	89614.616167	33.765453
857.035843	89774.501682	33.770471
857.859190	89923.525881	33.775488
858.660455	90088.381422	33.780506
859.756271	90247.525716	33.785524
860.778416	90403.772242	33.790541
861.871105	90552.129415	33.795559
863.201823	90707.573918	33.800576
863.708801	90855.580383	33.805594
864.448335	91010.865019	33.810612
865.816663	91164.743174	33.815629
866.279001	91315.398829	33.820647
867.492253	91472.949793	33.825664
868.651526	91617.961129	33.830682
869.375150	91757.716583	33.835700
870.256463	91902.699597	33.840717
871.184391	92055.611973	33.845735
871.931249	92199.619048	33.850752
872.966755	92340.800994	33.855770
873.556230	92486.905284	33.860788
874.655204	92623.078648	33.865805
875.087911	92788.538952	33.870823
875.885712	92939.554449	33.875840
877.088991	93097.586053	33.880858
877.486819	93258.112408	33.885876
878.528410	93407.128578	33.890893
879.332603	93557.146887	33.895911
880.385587	93720.182039	33.900928
881.100330	93876.369009	33.905946
881.737683	94050.905498	33.910964
882.784231	94194.862316	33.915981
884.084453	94351.025284	33.920999
884.904980	94505.920312	33.926016
885.909065	94658.937838	33.931034
886.685423	94811.512890	33.936052
887.696135	94964.929993	33.941069
888.176786	95109.599610	33.946087
889.315879	95258.338850	33.951104
890.033678	95400.667079	33.956122
890.687515	95545.000522	33.961140
891.907053	95685.715796	33.966157
892.777284	95842.408697	33.971175
893.576100	95986.986646	33.976192
894.242143	96134.334481	33.981210
894.850708	96293.098980	33.986228
895.798648	96440.060288	33.991245
896.357884	96615.697694	33.996263
897.063349	96762.017329	34.001280
898.253276	96930.602586	34.006298
899.260246	97110.575231	34.011316
900.241195	97258.795628	34.016333
900.830091	97426.078229	34.021351
901.617197	97584.859518	34.026368
902.441621	97762.145076	34.031386
903.479719	97944.061986	34.036404
904.496814	98107.948776	34.041421
905.336967	98280.829569	34.046439
906.185610	98452.558034	34.051456
907.468641	98617.524733	34.056474
908.422793	98791.599342	34.061492
909.809445	98947.511253	34.066509
910.560838	99119.671835	34.071527
911.467393	99288.446453	34.076544
912.346823	99455.675686	34.081562
913.167112	99619.117412	34.086580
914.247951	99789.069435	34.091597
914.735062	99955.765354	34.096615
915.770331	100134.488957	34.101632
917.104009	100302.940289	34.106650
917.665537	100477.085060	34.111668
919.038941	100647.830232	34.116685
919.691143	100820.423984	34.121703
920.616622	100986.832733	34.126720
922.086175	101148.885630	34.131738
922.637698	101322.746631	34.136756
923.439994	101489.647512	34.141773
924.559898	101659.460023	34.146791
925.733639	101830.619653	34.151808
926.410810	102001.672483	34.156826
927.208039	102166.983161	34.161844
928.491327	102347.954313	34.166861
928.984181	102512.285471	34.171879
929.863446	102687.868100	34.176896
930.814756	102857.975994	34.181914
931.902700	103042.783173	34.186932
932.945864	103212.859256	34.191949
933.919545	103383.904003	34.196967
934.704201	103553.816078	34.201984
935.820532	103728.131997	34.207002
936.736667	103904.767893	34.212020
937.936384	104074.728834	34.217037
939.059389	104242.417782	34.222055
939.669590	104420.899607	34.227072
940.897792	104585.185873	34.232090
941.818174	104755.355694	34.237108
942.756160	104923.560816	34.242125
943.612716	105089.336321	34.247143
944.435199	105258.069233	34.252160
945.281524	105428.375986	34.257178
946.240598	105598.665233	34.262196
947.424335	105756.950721	34.267213
948.266868	105942.331980	34.272231
949.680127	106100.518328	34.277248
950.338237	106269.835808	34.282266
951.091116	106430.374805	34.287284
952.251355	106595.052208	34.292301
953.336781	106758.818464	34.297319
953.806709	106918.330647	34.302336
954.926462	107073.329102	34.307354
955.963839	107227.164223	34.312372
956.747575	107389.033789	34.317389
957.342209	107553.291290	34.322407
958.093127	107727.364906	34.327424
959.294746	107893.107452	34.332442
959.964000	108069.349902	34.337460
961.559743	108228.380125	34.342477
962.069603	108393.518073	34.347495
963.358577	108569.788174	34.352512
964.126478	108738.229387	34.357530
965.130861	108901.414302	34.362548
966.215851	109075.770888	34.367565
967.121869	109245.497081	34.372583
968.027400	109427.599169	34.377600
968.969437	109601.235480	34.382618
969.944303	109769.813671	34.387636
971.044737	109945.287989	34.392653
972.293280	110108.186610	34.397671
973.079254	110297.280840	34.402688
974.586046	110464.090914	34.407706
975.385056	110646.687500	34.412724
976.332393	110812.287430	34.417741
977.365804	110989.527611	34.422759
978.356536	111166.155320	34.427776
979.264498	111328.319513	34.432794
980.433487	111507.909416	34.437812
981.001808	111681.392789	34.442829
982.020691	111868.103438	34.447847
982.474038	112050.728531	34.452864
983.833633	112218.929096	34.457882
984.776248	112409.975615	34.462900
985.820461	112589.390559	34.467917
987.019520	112773.632812	34.472935
987.667899	112961.096145	34.477952
988.588743	113146.425585	34.482970
989.837782	113337.275956	34.487988
990.249170	113534.105882	34.493005
991.226886	113719.201763	34.498023
991.972944	113926.987779	34.503040
993.324469	114106.665910	34.508058
994.338814	114305.922760	34.513076
995.066804	114506.697856	34.518093
996.284959	114700.387792	34.523111
997.141179	114912.166248	34.528128
997.909497	115099.991660	34.533146
998.869500	115315.455302	34.538164
999.790431	115519.537734	34.543181
1001.195918	115714.952095	34.548199
1002.041290	115923.078676	34.553216
1003.072830	116134.723428	34.558234
1003.905894	116336.406506	34.563252
1004.916159	116549.742905	34.568269
1006.082901	116744.849109	34.573287
1006.666254	116960.945022	34.578304
1007.844880	117157.319067	34.583322
1008.864159	117380.225814	34.588340
1010.141100	117590.840068	34.593357
1010.929806	117798.026930	34.598375
1011.951519	118015.756278	34.603392
1013.177116	118212.269242	34.608410
1014.256228	118421.034463	34.613428
1015.202256	118624.070882	34.618445
1016.893315	118831.483718	34.623463
1017.382187	119030.835403	34.628480
1018.548532	119224.210167	34.633498
1019.587622	119404.784581	34.638516
1020.569319	119599.801526	34.643533
1021.668194	119782.319728	34.648551
1022.350875	119985.941431	34.653568
1023.142090	120181.893394	34.658586
1024.328241	120376.539720	34.663604
1024.604690	120586.732963	34.668621
1026.023131	120779.734416	34.673639
1027.016197	121000.760278	34.678656
1028.078487	121207.977233	34.683674
1028.965020	121410.156083	34.688692
1029.949925	121618.706569	34.693709
1031.100848	121822.124453	34.698727
1031.749414	122048.385170	34.703744
1033.114108	122262.351746	34.708762
1034.097814	122478.942516	34.713780
1034.848681	122698.982103	34.718797
1036.365132	122912.053985	34.723815
1037.067467	123140.493836	34.728832
1037.976873	123358.814091	34.733850
1038.604509	123589.880245	34.738868
1039.784615	123817.232649	34.743885
1041.178283	124039.811976	34.748903
1041.975693	124283.033885	34.753920
1043.369617	124506.300987	34.758938
1044.822480	124732.563510	34.763956
1045.737578	124955.418778	34.768973
1047.300549	125176.014318	34.773991
1048.137906	125401.293626	34.779008
1049.145564	125609.843115	34.784026
1050.157764	125841.610926	34.789044
1050.805339	126070.804632	34.794061
1052.572683	126288.523061	34.799079
1053.109324	126522.516443	34.804096
1054.350732	126754.912450	34.809114
1055.595596	126980.161610	34.814132
1056.170680	127211.619185	34.819149
1057.518223	127446.550424	34.824167
1058.120531	127683.317513	34.829184
1059.502061	127910.515481	34.834202
1060.574707	128147.918276	34.839220
1061.223972	128371.019993	34.844237
1062.712077	128610.689875	34.849255
1063.833605	128841.879443	34.854272
1064.766073	129076.169239	34.859290
1066.350000	129325.677124	34.864308
1067.356599	129549.514215	34.869325
1068.671203	129768.384170	34.874343
1069.739893	130006.270891	34.879360
1071.022459	130232.868547	34.884378
1071.826403	130456.593524	34.889396
1072.792183	130688.164797	34.894413
1074.525692	130915.098573	34.899431
1075.101490	131153.873965	34.904448
1075.838497	131371.912528	34.909466
1076.880553	131606.177903	34.914484
1077.806500	131842.619082	34.919501
1079.068820	132079.298049	34.924519
1079.697334	132317.769334	34.929536
1081.140212	132552.660064	34.934554
1082.688745	132781.830792	34.939572
1083.747750	133007.268417	34.944589
1084.685315	133240.143382	34.949607
1086.198456	133472.912350	34.954624
1087.345228	133693.751446	34.959642
1088.434406	133935.809652	34.964660
1089.552681	134150.090078	34.969677
1090.831035	134359.021230	34.974695
1091.735807	134567.330858	34.979712
1092.454603	134781.719467	34.984730
1093.920423	134989.749046	34.989748
1094.389726	135208.453853	34.994765
1095.803097	135425.267499	34.999783
1096.420506	135652.115006	35.004800
1097.284007	135867.627869	35.009818
1098.564591	136092.873029	35.014836
1099.984510	136322.140901	35.019853
1100.574232	136544.333820	35.024871
1101.366889	136783.102647	35.029888
1102.444941	137023.246019	35.034906
1103.639235	137262.268970	35.039924
1104.442103	137502.131636	35.044941
1105.410029	137747.661289	35.049959
1106.582622	138008.043252	35.054976
1107.278299	138255.738884	35.059994
1108.331886	138522.344243	35.065012
1109.236082	138780.431051	35.070029
1110.691879	139036.019851	35.075047
1111.575606	139302.989132	35.080064
1112.290280	139562.241667	35.085082
1113.789787	139836.023510	35.090100
1114.599099	140115.829959	35.095117
1115.676741	140384.931255	35.100135
1117.005882	140663.781565	35.105152
1118.461009	140922.757486	35.110170
1119.841103	141201.515049	35.115188
1121.316006	141468.061500	35.120205
1122.489013	141720.078261	35.125223
1122.987140	141996.756295	35.130240
1123.915159	142262.093198	35.135258
1125.671697	142535.030151	35.140276
1126.507732	142812.356365	35.145293
1127.792418	143085.261448	35.150311
1128.919562	143360.286933	35.155328
1129.782633	143631.604804	35.160346
1131.202603	143909.769071	35.165364
1132.224325	144192.426819	35.170381
1133.085345	144474.111608	35.175399
1134.212033	144762.260040	35.180416
1135.209581	145041.035628	35.185434
1136.157050	145327.214698	35.190452
1137.638682	145606.231870	35.195469
1138.613597	145898.383822	35.200487
1140.184865	146191.771270	35.205504
1141.088876	146476.647947	35.210522
1142.624940	146766.089350	35.215540
1143.551572	147054.936213	35.220557
1144.649373	147353.585461	35.225575
1145.737569	147633.482399	35.230592
1146.628599	147928.530878	35.235610
1147.849327	148214.485078	35.240628
1148.414366	148504.531953	35.245645
1149.858035	148795.983332	35.250663
1151.015504	149096.247763	35.255680
1152.020860	149406.990081	35.260698
1153.845580	149712.539457	35.265716
1155.035611	149997.967369	35.270733
1156.012664	150298.563136	35.275751
1157.192793	150591.315211	35.280768
1158.256076	150894.260595	35.285786
1159.641727	151183.356107	35.290804
1160.319524	151484.847979	35.295821
1161.453723	151774.737894	35.300839
1162.838039	152078.274076	35.305856
1163.596646	152395.233606	35.310874
1165.386613	152661.963657	35.315892
1166.522217	152945.292314	35.320909
1167.972843	153232.274738	35.325927
1168.975705	153507.968556	35.330944
1169.513041	153797.985241	35.335962
1171.324318	154079.599976	35.340980
1172.243090	154369.989299	35.345997
1173.553000	154648.380436	35.351015
1174.900475	154931.308362	35.356032
1175.768957	155225.416261	35.361050
1176.890592	155511.011385	35.366068
1178.221034	155813.292403	35.371085
1179.243988	156093.035147	35.376103
1180.582692	156397.691375	35.381120
1181.576895	156695.404806	35.386138
1182.896092	156982.830099	35.391156
1183.818148	157283.870675	35.396173
1185.143368	157574.572039	35.401191
1186.276229	157888.254882	35.406208
1187.148420	158186.177309	35.411226
1188.771404	158488.227654	35.416244
1189.950544	158806.692513	35.421261
1190.877953	159103.153840	35.426279
1192.543566	159411.280537	35.431296
1193.560705	159717.030218	35.436314
1194.902003	160019.176650	35.441332
1196.011011	160324.230719	35.446349
1197.312203	160635.776015	35.451367
1198.753799	160934.766552	35.456384
1199.564303	161250.381004	35.461402
1200.912492	161568.763570	35.466420
1201.997159	161879.047374	35.471437
1203.304015	162197.200578	35.476455
1204.440945	162507.607342	35.481472
1206.018213	162821.077376	35.486490
1207.165709	163132.057962	35.491508
1207.884423	163450.279777	35.496525
1209.191394	163775.575098	35.501543
1210.564204	164090.940706	35.506560
1211.677412	164418.429792	35.511578
1213.129163	164721.543871	35.516596
1214.380865	165050.410586	35.521613
1215.761079	165359.618308	35.526631
1217.135613	165665.162480	35.531648
1218.540357	165990.585505	35.536666
1219.866020	166301.775621	35.541684
1220.701189	166609.712023	35.546701
1222.178920	166934.660662	35.551719
1223.340453	167229.326691	35.556736
1224.319019	167562.558915	35.561754
1225.603315	167881.164376	35.566772
1226.719245	168206.410580	35.571789
1227.949803	168523.405450	35.576807
1229.350814	168839.232487	35.581824
1230.329072	169161.513939	35.586842
1231.863242	169479.518680	35.591860
1232.530367	169801.818046	35.596877
1234.038961	170132.101739	35.601895
1235.604754	170443.953972	35.606912
1236.217435	170770.202847	35.611930
1237.669320	171102.596697	35.616948
1239.044395	171424.613131	35.621965
1240.085314	171755.709134	35.626983
1241.421386	172073.549079	35.632000
1242.372945	172400.108960	35.637018
1243.406043	172736.669817	35.642036
1244.913814	173077.304310	35.647053
1246.089104	173401.727819	35.652071
1247.353741	173715.047851	35.657088
1248.374977	174044.412237	35.662106
1249.392745	174365.226383	35.667124
1250.746851	174691.317062	35.672141
1251.676643	175014.167863	35.677159
1253.213134	175330.512089	35.682176
1254.532796	175660.599861	35.687194
1255.749858	175982.648363	35.692212
1257.350742	176313.506395	35.697229
1258.561541	176637.210078	35.702247
1259.968822	176950.730875	35.707264
1260.738218	177283.763289	35.712282
1262.213328	177605.196188	35.717300
1263.780049	177953.178382	35.722317
1264.926910	178287.665533	35.727335
1265.862648	178616.770648	35.732352
1266.938079	178961.198646	35.737370
1268.129235	179307.767451	35.742388
1269.408065	179650.808647	35.747405
1270.630378	179999.344257	35.752423
1271.699130	180343.224402	35.757440
1272.550498	180703.007406	35.762458
1274.205352	181056.784020	35.767476
1275.468963	181414.980974	35.772493
1276.520865	181777.061037	35.777511
1277.729688	182140.272712	35.782528
1278.558052	182520.912608	35.787546
1280.040938	182885.188462	35.792564
1281.591115	183256.347684	35.797581
1282.576664	183645.067509	35.802599
1283.758077	184017.308337	35.807616
1285.493281	184399.677922	35.812634
1286.511150	184773.271050	35.817652
1288.161861	185141.101335	35.822669
1289.169113	185524.906433	35.827687
1290.594440	185907.096696	35.832704
1292.078010	186285.852896	35.837722
1293.622549	186671.836744	35.842740
1295.022620	187049.609227	35.847757
1296.246505	187425.991712	35.852775
1297.782410	187803.911917	35.857792
1298.971211	188184.544904	35.862810
1300.246948	188564.201402	35.867828
1302.387376	188938.944912	35.872845
1303.484476	189311.375119	35.877863
1304.903274	189662.581351	35.882880
1306.453370	190036.794802	35.887898
1307.948696	190397.526009	35.892916
1309.549603	190755.652441	35.897933
1310.278338	191131.849153	35.902951
1311.594422	191485.025565	35.907968
1313.202751	191864.890054	35.912986
1314.543569	192224.121980	35.918004
1315.811592	192587.887311	35.923021
1317.002142	192953.825707	35.928039
1318.908898	193323.976979	35.933056
1320.056395	193692.732464	35.938074
1321.297590	194061.093872	35.943092
1322.461632	194423.986057	35.948109
1323.768109	194797.812583	35.953127
1325.039635	195145.152687	35.958144
1326.202687	195510.361887	35.963162
1327.633397	195877.369833	35.968180
1328.938798	196258.454199	35.973197
1330.357588	196629.619817	35.978215
1331.552265	196985.412420	35.983232
1332.372804	197365.136155	35.988250
1333.978773	197726.006624	35.993268
1335.548703	198083.749244	35.998285
1336.454627	198448.382889	36.003303
1338.131009	198791.194429	36.008320
1338.904325	199152.819590	36.013338
1340.327250	199502.088014	36.018356
1342.451297	199856.447874	36.023373
1343.773388	200203.667169	36.028391
1345.337566	200555.583918	36.033408
1346.521670	200902.842268	36.038426
1347.762976	201254.016059	36.043444
1349.157967	201612.263478	36.048461
1350.481123	201979.919876	36.053479
1351.648356	202333.193568	36.058496
1352.864630	202693.304328	36.063514
1354.229398	203056.261831	36.068532
1355.538868	203423.547152	36.073549
1356.504442	203795.233369	36.078567
1357.898480	204163.549655	36.083584
1359.092877	204537.601613	36.088602
1360.300798	204925.391231	36.093620
1361.543800	205322.763271	36.098637
1362.791175	205702.551431	36.103655
1364.226372	206090.804847	36.108672
1365.613910	206481.759928	36.113690
1366.843307	206880.767744	36.118708
1368.365815	207272.390283	36.123725
1369.611161	207673.850183	36.128743
1371.078536	208068.444352	36.133760
1372.396657	208467.712416	36.138778
1373.478279	208878.271525	36.143796
1375.194169	209274.176693	36.148813
1376.299004	209682.894998	36.153831
1377.877121	210089.619928	36.158848
1379.567950	210503.959652	36.163866
1380.505874	210915.137009	36.168884
1382.341843	211320.111327	36.173901
1383.682781	211737.537117	36.178919
1384.909393	212154.260075	36.183936
1386.228850	212558.195522	36.188954
1387.403664	212984.962592	36.193972
1389.302055	213390.558778	36.198989
1390.328627	213808.033928	36.204007
1391.673916	214231.502872	36.209024
1393.206840	214649.965127	36.214042
1394.634692	215078.148295	36.219060
1395.961747	215491.111958	36.224077
1397.337667	215922.507731	36.229095
1398.999429	216348.093201	36.234112
1400.498212	216773.377368	36.239130
1401.517522	217199.707711	36.244148
1403.402329	217608.296644	36.249165
1405.036881	218037.424555	36.254183
1406.539881	218520.647989	36.259200
1408.276569	218941.305603	36.264218
1409.563689	219351.854615	36.269236
1411.043397	219769.307235	36.274253
1412.200396	220188.999102	36.279271
1413.408741	220603.985550	36.284288
1415.040536	221016.770336	36.289306
1415.986698	221446.737741	36.294324
1417.545641	221872.465813	36.299341
1418.847919	222289.551595	36.304359
1420.250964	222727.805013	36.309376
1421.624343	223153.035453	36.314394
1423.304690	223579.969427	36.319412
1424.902537	223993.660322	36.324429
1426.081382	224428.554060	36.329447
1427.690064	224833.483532	36.334464
1429.480801	225247.121796	36.339482
1431.048982	225650.892464	36.344500
1433.070452	226024.288016	36.349517
1434.594552	226422.912502	36.354535
1435.763709	226805.671249	36.359552
1437.414850	227200.543589	36.364570
1438.617544	227577.076276	36.369588
1439.929769	227961.516831	36.374605
1441.088649	228374.482754	36.379623
1442.503604	228769.094254	36.384640
1443.403231	229154.901932	36.389658
1444.862947	229573.384723	36.394676
1447.074052	229975.996607	36.399693
1448.184267	230391.720221	36.404711
1448.972170	230797.007880	36.409728
1450.816432	231208.421766	36.414746
1451.908879	231629.537001	36.419764
1453.803636	232043.510483	36.424781
1455.145453	232475.230000	36.429799
1456.514319	232884.110914	36.434816
1458.197631	233314.608115	36.439834
1459.286867	233737.711280	36.444852
1460.712086	234168.888540	36.449869
1461.938351	234608.685444	36.454887
1463.325500	235042.335324	36.459904
1465.006302	235478.097038	36.464922
1466.371539	235917.518997	36.469940
1467.468300	236356.046574	36.474957
1469.106817	236792.453770	36.479975
1470.726428	237255.765500	36.484992
1472.449995	237687.004393	36.490010
1473.497588	238143.503597	36.495028
1474.813794	238575.523093	36.500045
1476.622176	239036.572906	36.505063
1478.044709	239502.793302	36.510080
1479.855650	239936.537803	36.515098
1481.462280	240398.157603	36.520116
1483.257469	240849.561104	36.525133
1484.226443	241302.727672	36.530151
1485.851554	241756.828426	36.535168
1487.487099	242217.482194	36.540186
1488.531823	242678.107404	36.545204
1490.488655	243132.384857	36.550221
1491.611334	243601.381827	36.555239
1492.656256	244063.051236	36.560256
1494.508947	244529.871933	36.565274
1495.759151	245006.217257	36.570292
1497.500125	245464.776856	36.575309
1498.665803	245944.135320	36.580327
1500.260876	246418.876672	36.585344
1501.892505	246887.516124	36.590362
1503.157552	247377.656738	36.595380
1505.047527	247846.382060	36.600397
1506.626436	248316.963002	36.605415
1508.171737	248785.416317	36.610432
1510.001890	249254.966395	36.615450
1511.365165	249729.471494	36.620468
1512.992329	250202.231651	36.625485
1514.238474	250675.436297	36.630503
1515.851134	251140.909295	36.635520
1517.765092	251612.709245	36.640538
1519.261758	252083.460812	36.645556
1520.801386	252559.896049	36.650573
1522.660952	253026.320916	36.655591
1523.715803	253501.795482	36.660608
1525.236191	253955.245285	36.665626
1526.563731	254431.285278	36.670644
1528.017538	254896.762450	36.675661
1529.279613	255353.710679	36.680679
1530.908427	255812.986566	36.685696
1532.441687	256264.835319	36.690714
1533.603565	256734.324629	36.695732
1535.195221	257191.524259	36.700749
1537.028059	257648.989108	36.705767
1539.029442	258099.160958	36.710784
1540.851689	258555.484688	36.715802
1542.330910	259019.460715	36.720820
1543.493058	259481.812529	36.725837
1545.012082	259930.641763	36.730855
1546.347825	260403.659823	36.735872
1548.243294	260868.685107	36.740890
1549.495575	261338.439913	36.745908
1550.925060	261799.325091	36.750925
1552.550706	262280.983144	36.755943
1553.392370	262752.532940	36.760960
1555.295242	263237.803113	36.765978
1556.768489	263735.947280	36.770996
1558.483373	264216.548536	36.776013
1559.500770	264709.991712	36.781031
1560.809644	265210.575668	36.786048
1562.681687	265714.673676	36.791066
1563.947993	266218.668094	36.796084
1566.030845	266728.649601	36.801101
1567.569029	267220.989178	36.806119
1568.934077	267729.538743	36.811136
1571.083391	268217.381916	36.816154
1572.514925	268735.572782	36.821172
1574.152001	269245.752634	36.826189
1575.646566	269749.604690	36.831207
1576.830088	270269.536811	36.836224
1578.974803	270774.906200	36.841242
1580.312210	271285.488757	36.846260
1581.928543	271808.294221	36.851277
1583.879100	272326.115633	36.856295
1585.032404	272851.790291	36.861312
1586.720726	273350.956927	36.866330
1588.187810	273881.506306	36.871348
1589.653630	274413.731561	36.876365
1591.246717	274937.678994	36.881383
1593.024351	275456.539894	36.886400
1594.332563	275985.104850	36.891418
1596.357945	276515.658833	36.896436
1597.434644	277047.994015	36.901453
1599.208580	277572.998729	36.906471
1600.676625	278119.136732	36.911488
1602.188066	278651.193426	36.916506
1604.018593	279195.592516	36.921524
1605.506168	279743.526946	36.926541
1606.846332	280275.557173	36.931559
1607.924584	280833.132906	36.936576
1610.241711	281372.695910	36.941594
1611.843343	281922.307636	36.946612
1613.637158	282469.498307	36.951629
1615.766785	283007.512741	36.956647
1617.370030	283563.114199	36.961664
1619.234006	284086.512482	36.966682
1621.025790	284623.536321	36.971700
1622.673356	285164.036859	36.976717
1624.153702	285690.998909	36.981735
1625.643081	286233.731959	36.986752
1627.541882	286773.576080	36.991770
1628.808769	287308.112166	36.996788
1630.286396	287851.298762	37.001805
1631.928330	288388.207659	37.006823
1633.688026	288942.316925	37.011840
1635.455887	289468.786730	37.016858
1637.018268	289993.180229	37.021876
1638.603619	290518.253779	37.026893
1640.386659	291026.299802	37.031911
1642.029238	291551.334508	37.036928
1643.411947	292049.434951	37.041946
1644.876485	292593.265639	37.046964
1646.635598	293112.534384	37.051981
1647.962568	293643.810250	37.056999
1649.318995	294182.419524	37.062016
1651.036724	294716.471057	37.067034
1652.439899	295252.959672	37.072052
1654.190516	295804.374211	37.077069
1655.804252	296343.286839	37.082087
1657.217588	296900.898425	37.087104
1659.057052	297450.969609	37.092122
1660.649628	298003.771093	37.097140
1662.194747	298579.766752	37.102157
1664.210672	299125.812778	37.107175
1665.503672	299683.658613	37.112192
1667.009138	300259.423114	37.117210
1669.180548	300815.695631	37.122228
1670.708160	301392.034270	37.127245
1672.573749	301954.827494	37.132263
1673.975982	302535.624851	37.137280
1675.695531	303102.016692	37.142298
1677.844675	303680.804521	37.147316
1679.339632	304258.985624	37.152333
1681.338101	304819.276620	37.157351
1682.841063	305408.116105	37.162368
1684.673693	305972.973501	37.167386
1686.574977	306545.511248	37.172404
1688.596291	307120.108029	37.177421
1689.938979	307699.485958	37.182439
1691.338654	308293.351881	37.187456
1692.782505	308867.753005	37.192474
1694.507909	309450.306660	37.197492
1696.074424	310051.167397	37.202509
1698.221091	310638.798557	37.207527
1699.471681	311230.382630	37.212544
1701.432217	311832.993720	37.217562
1702.951902	312426.454614	37.222580
1704.838796	313024.015204	37.227597
1706.953988	313612.696233	37.232615
1708.492496	314212.031976	37.237632
1709.962767	314807.946049	37.242650
1712.079995	315419.721496	37.247668
1713.425524	316012.370752	37.252685
1715.375411	316612.990697	37.257703
1717.474236	317211.219542	37.262720
1719.298066	317807.101841	37.267738
1720.791074	318414.181248	37.272756
1722.414070	318996.272950	37.277773
1724.471420	319595.377311	37.282791
1725.785575	320198.661866	37.287808
1727.392643	320796.103399	37.292826
1729.540033	321402.820120	37.297844
1731.186642	322002.326589	37.302861
1733.142749	322612.517149	37.307879
1735.124635	323204.492355	37.312896
1737.238406	323796.465823	37.317914
1739.201178	324389.525189	37.322932
1740.425597	324982.116894	37.327949
1742.463304	325562.635493	37.332967
1743.978022	326164.384860	37.337984
1746.016917	326753.143958	37.343002
1747.783363	327344.887570	37.348020
1748.575409	327935.262857	37.353037
1750.556985	328518.682687	37.358055
1752.361869	329115.810536	37.363072
1753.605943	329697.055566	37.368090
1755.721104	330273.403574	37.373108
1757.292762	330862.656511	37.378125
1759.107292	331434.675913	37.383143
1760.851307	332015.383791	37.388160
1762.769287	332600.601383	37.393178
1764.471965	333187.422446	37.398196
1766.002487	333776.169791	37.403213
1767.944232	334366.010858	37.408231
1769.535070	334955.345034	37.413248
1771.216057	335554.533117	37.418266
1773.434647	336146.619498	37.423284
1775.195287	336742.430423	37.428301
1776.620176	337339.127823	37.433319
1778.442015	337936.616127	37.438336
1780.081558	338542.504609	37.443354
1781.900698	339158.713188	37.448372
1783.494330	339770.737943	37.453389
1785.220253	340389.536400	37.458407
1786.505147	341013.603690	37.463424
1788.082443	341642.412444	37.468442
1790.044508	342264.474250	37.473460
1792.070677	342908.270350	37.478477
1793.810367	343535.987815	37.483495
1795.690553	344170.603278	37.488512
1797.295224	344817.667395	37.493530
1799.442455	345450.902276	37.498548
1800.890195	346113.051201	37.503565
1802.906622	346746.595099	37.508583
1804.514847	347398.420643	37.513600
1806.339107	348052.257256	37.518618
1808.451265	348702.737917	37.523636
1809.887432	349365.375905	37.528653
1812.026507	350021.010820	37.533671
1813.860562	350684.249307	37.538688
1815.654853	351345.961976	37.543706
1817.405531	351995.567098	37.548724
1819.452358	352673.053976	37.553741
1821.113924	353320.091375	37.558759
1822.751562	353996.077478	37.563776
1824.496860	354663.991223	37.568794
1826.251454	355346.813900	37.573812
1827.756628	356041.618526	37.578829
1829.826867	356704.828751	37.583847
1831.482164	357393.928009	37.588864
1833.370886	358080.566982	37.593882
1835.236655	358755.247610	37.598900
1837.296745	359449.549272	37.603917
1839.282240	360129.845915	37.608935
1841.122061	360823.450277	37.613952
1842.919817	361514.487213	37.618970
1845.232899	362195.380312	37.623988
1846.659686	362890.793305	37.629005
1848.855698	363562.954873	37.634023
1850.926240	364264.148929	37.639040
1852.463456	364954.331997	37.644058
1854.513131	365645.813635	37.649076
1856.052378	366334.322919	37.654093
1858.232815	367028.396598	37.659111
1859.930542	367715.282172	37.664128
1861.748292	368415.377225	37.669146
1863.973594	369098.903712	37.674164
1865.620685	369787.890785	37.679181
1867.740521	370473.920824	37.684199
1869.559067	371165.847260	37.689216
1871.195819	371850.206604	37.694234
1873.394524	372520.231047	37.699252
1875.192848	373199.440209	37.704269
1877.162613	373856.212423	37.709287
1878.870970	374528.208189	37.714304
1880.436611	375181.370528	37.719322
1882.787277	375843.394901	37.724340
1884.290550	376523.680161	37.729357
1885.880746	377188.924167	37.734375
1887.645235	377874.820985	37.739392
1889.457877	378555.979341	37.744410
1891.137708	379240.721866	37.749428
1892.955127	379934.531937	37.754445
1894.643515	380619.499057	37.759463
1896.537811	381314.434803	37.764480
1898.444408	382014.501775	37.769498
1900.222030	382716.730748	37.774516
1901.767098	383436.276368	37.779533
1903.416208	384152.543657	37.784551
1905.296727	384872.560503	37.789568
1906.884914	385613.425984	37.794586
1908.923686	386344.033271	37.799604
1910.598981	387081.909793	37.804621
1912.710753	387834.757080	37.809639
1915.055159	388569.928360	37.814656
1916.827230	389320.210671	37.819674
1919.052776	390062.642909	37.824692
1921.042638	390807.378040	37.829709
1922.993682	391562.393923	37.834727
1924.978921	392301.238263	37.839744
1926.724662	393057.341601	37.844762
1928.750296	393806.662903	37.849780
1930.554930	394568.371860	37.854797
1932.647340	395326.060131	37.859815
1934.780290	396097.358973	37.864832
1935.933026	396860.308908	37.869850
1938.267243	397640.481777	37.874868
1940.081367	398414.510579	37.879885
1942.084822	399186.561737	37.884903
1943.959593	399968.396172	37.889920
1945.580056	400751.620085	37.894938
1948.162199	401532.738276	37.899956
1949.825690	402318.421486	37.904973
1951.950275	403096.886542	37.909991
1953.795294	403883.839848	37.915008
1955.813942	404686.984828	37.920026
1957.788697	405464.016007	37.925044
1959.802533	406264.304228	37.930061
1961.750129	407064.099025	37.935079
1964.314052	407859.690037	37.940096
1965.912950	408651.971698	37.945114
1968.315874	409435.636184	37.950132
1970.551477	410233.923298	37.955149
1972.419132	411022.950444	37.960167
1974.546303	411798.181685	37.965184
1976.162337	412603.391309	37.970202
1977.830219	413401.044911	37.975220
1979.765675	414205.317545	37.980237
1981.954679	414999.772173	37.985255
1983.960829	415793.194499	37.990272
1985.943484	416585.127640	37.995290
1987.964009	417386.907909	38.000308
1989.929451	418182.011687	38.005325
1992.254335	418977.082293	38.010343
1994.771213	419775.388750	38.015360
1996.484727	420563.825180	38.020378
1998.495151	421344.844498	38.025396
2001.053558	422136.941656	38.030413
2002.908225	422920.951118	38.035431
2005.157409	423690.666102	38.040448
2006.948660	424446.582884	38.045466
2009.159945	425205.597510	38.050484
2010.997076	425954.675090	38.055501
2012.535876	426705.449955	38.060519
2014.864945	427470.603170	38.065536
2016.254759	428235.937838	38.070554
2018.043933	428999.461013	38.075572
2020.472324	429774.347225	38.080589
2021.701185	430550.266879	38.085607
2023.610710	431321.999030	38.090624
2025.744268	432118.322814	38.095642
2027.438802	432909.326267	38.100660
2029.120206	433711.137994	38.105677
2030.993635	434516.585739	38.110695
2032.917359	435325.591132	38.115712
2034.817592	436148.187564	38.120730
2037.007695	436976.982887	38.125748
2039.128332	437793.410652	38.130765
2041.144126	438633.461109	38.135783
2043.167024	439453.995525	38.140800
2044.980692	440298.319356	38.145818
2046.944400	441142.485615	38.150836
2048.964349	441992.278235	38.155853
2050.705446	442843.147102	38.160871
2053.120370	443691.848349	38.165888
2054.920886	444555.291174	38.170906
2057.095699	445429.465499	38.175924
2059.514632	446285.452783	38.180941
2061.906734	447157.043161	38.185959
2064.222381	448003.418376	38.190976
2066.530331	448868.630230	38.195994
2068.705454	449733.525664	38.201012
2071.257020	450565.496452	38.206029
2073.390641	451441.052903	38.211047
2075.924288	452286.261747	38.216064
2077.761180	453147.078393	38.221082
2079.744358	453992.714131	38.226100
2082.200240	454835.810287	38.231117
2083.883060	455699.885014	38.236135
2086.242286	456542.270455	38.241152
2088.096250	457413.830475	38.246170
2089.989444	458267.043185	38.251188
2092.112880	459135.603463	38.256205
2093.977050	460003.967216	38.261223
2096.440951	460865.167484	38.266240
2098.220616	461749.446165	38.271258
2100.245708	462631.572813	38.276276
2102.712076	463497.310659	38.281293
2104.584979	464375.897354	38.286311
2107.059472	465230.589448	38.291328
2108.961568	466116.119900	38.296346
2111.059167	466990.004294	38.301364
2113.159172	467876.382914	38.306381
2114.711733	468764.630809	38.311399
2117.196169	469657.586185	38.316416
2119.096796	470544.229530	38.321434
2121.359814	471432.742890	38.326452
2123.598765	472322.633750	38.331469
2125.513748	473215.972187	38.336487
2128.200006	474105.402731	38.341504
2129.988334	474993.322851	38.346522
2132.270441	475889.758184	38.351540
2134.217170	476776.355463	38.356557
2136.138600	477671.350448	38.361575
2139.082618	478559.264275	38.366592
2140.967947	479445.794835	38.371610
2143.166941	480335.362369	38.376628
2145.626354	481218.379434	38.381645
2147.174364	482083.677371	38.386663
2149.317011	482939.897911	38.391680
2151.368767	483811.595264	38.396698
2153.812922	484676.116737	38.401716
2156.027963	485528.314601	38.406733
2158.072187	486394.788398	38.411751
2160.175039	487259.544409	38.416768
2162.307736	488137.985007	38.421786
2164.467358	489001.637055	38.426804
2166.896185	489862.375601	38.431821
2168.877083	490743.033491	38.436839
2170.642061	491627.619616	38.441856
2173.002426	492502.220792	38.446874
2174.847525	493397.605464	38.451892
2176.262275	494284.839260	38.456909
2178.163211	495213.983122	38.461927
2180.386349	496115.320692	38.466944
2182.686431	497038.950868	38.471962
2184.889258	497966.179717	38.476980
2187.094813	498892.651057	38.481997
2188.952101	499818.674934	38.487015
2191.146886	500760.936909	38.492032
2193.377036	501701.424938	38.497050
2195.421393	502657.880373	38.502068
2198.059429	503595.218104	38.507085
2200.085603	504552.424669	38.512103
2202.342491	505502.224900	38.517120
2204.576840	506459.639138	38.522138
2206.468688	507430.366336	38.527156
2208.659578	508390.195738	38.532173
2210.788459	509363.339939	38.537191
2213.091498	510337.657206	38.542208
2215.136235	511324.158278	38.547226
2217.167065	512313.675960	38.552244
2219.520601	513296.828460	38.557261
2221.622884	514303.954235	38.562279
2224.158566	515292.850268	38.567296
2226.725624	516281.679059	38.572314
2228.580069	517277.064037	38.577332
2231.231834	518277.847676	38.582349
2233.480931	519286.796348	38.587367
2235.783577	520275.818652	38.592384
2237.665145	521280.969374	38.597402
2240.197866	522286.198944	38.602420
2242.563587	523291.390088	38.607437
2244.682270	524309.501425	38.612455
2246.849176	525306.129821	38.617472
2249.380561	526313.360383	38.622490
2251.999186	527330.279541	38.627508
2254.402673	528334.424535	38.632525
2256.449937	529351.804338	38.637543
2259.201188	530344.024018	38.642560
2261.883188	531336.994360	38.647578
2263.975189	532345.602326	38.652596
2265.979464	533342.879139	38.657613
2267.959927	534356.552746	38.662631
2270.772605	535360.455221	38.667648
2272.733530	536356.778544	38.672666
2274.941733	537370.355802	38.677684
2277.151343	538371.834215	38.682701
2279.423011	539389.536688	38.687719
2281.750880	540383.961404	38.692736
2284.519760	541399.375985	38.697754
2286.157145	542417.369885	38.702772
2288.922245	543412.617738	38.707789
2291.082588	544427.664277	38.712807
2293.174543	545428.917163	38.717824
2295.773066	546440.225087	38.722842
2297.537314	547432.938967	38.727860
2299.784472	548406.996224	38.732877
2302.138627	549400.729484	38.737895
2304.546918	550376.431882	38.742912
2306.723241	551353.963684	38.747930
2308.975437	552345.741533	38.752948
2311.213665	553329.456721	38.757965
2313.527419	554326.007067	38.762983
2315.532718	555323.892240	38.768000
2317.759719	556318.500913	38.773018
2319.759261	557336.392426	38.778036
2321.946215	558350.859287	38.783053
2324.072793	559375.459598	38.788071
2326.199061	560409.979861	38.793088
2328.528713	561445.541586	38.798106
2331.085836	562489.524997	38.803124
2333.358959	563532.869824	38.808141
2335.540327	564580.315923	38.813159
2337.744942	565637.116594	38.818176
2340.258106	566688.608127	38.823194
2342.126102	567752.172870	38.828212
2344.474058	568830.584557	38.833229
2346.623570	569916.269186	38.838247
2349.094921	571002.110314	38.843264
2351.319582	572083.984542	38.848282
2353.599851	573177.503527	38.853300
2355.990602	574280.797816	38.858317
2358.381295	575381.988593	38.863335
2360.644222	576499.413449	38.868352
2363.109108	577601.502000	38.873370
2365.489815	578722.422666	38.878388
2368.201229	579833.054147	38.883405
2370.745591	580954.850686	38.888423
2373.047734	582077.187506	38.893440
2375.728036	583191.184722	38.898458
2378.159821	584310.889280	38.903476
2380.536597	585432.255695	38.908493
2382.884458	586550.715993	38.913511
2385.401560	587683.384553	38.918528
2387.932226	588812.586206	38.923546
2389.972103	589957.503031	38.928564
2392.323112	591086.070175	38.933581
2394.569761	592222.567068	38.938599
2396.634374	593365.500478	38.943616
2398.836296	594513.713131	38.948634
2401.330385	595663.820650	38.953652
2403.776698	596825.997884	38.958669
2406.378924	597991.691448	38.963687
2408.621566	599153.321373	38.968704
2411.387175	600297.220521	38.973722
2414.046760	601455.948026	38.978740
2416.316063	602625.840485	38.983757
2418.759271	603789.978240	38.988775
2421.115015	604954.563418	38.993792
2423.912869	606128.768835	38.998810
2426.238666	607290.468344	39.003828
2428.831469	608440.444361	39.008845
2431.198485	609605.604057	39.013863
2433.738620	610783.074468	39.018880
2436.307052	611938.002804	39.023898
2438.782916	613116.490355	39.028916
2441.469109	614266.156690	39.033933
2443.970381	615441.143349	39.038951
2445.827801	616586.655280	39.043968
2448.774012	617757.772352	39.048986
2451.189606	618911.202321	39.054004
2453.660834	620064.652101	39.059021
2456.141455	621219.178669	39.064039
2458.459160	622365.812367	39.069056
2461.392360	623484.385048	39.074074
2463.260747	624617.310631	39.079092
2465.899867	625734.350008	39.084109
2468.099499	626869.832762	39.089127
2470.154446	628000.872876	39.094144
2472.971460	629134.565143	39.099162
2474.874534	630287.667475	39.104180
2476.953385	631425.782760	39.109197
2479.757125	632575.791093	39.114215
2481.315520	633756.837231	39.119232
2483.934592	634931.784558	39.124250
2486.119335	636118.253428	39.129268
2488.233588	637309.191413	39.134285
2490.811215	638501.164585	39.139303
2492.991518	639719.365444	39.144320
2495.339006	640928.513553	39.149338
2497.451534	642168.042286	39.154356
2499.794300	643398.104822	39.159373
2502.615081	644635.123393	39.164391
2504.586680	645876.770150	39.169408
2507.006384	647131.805138	39.174426
2509.674224	648405.391431	39.179444
2511.981893	649675.585984	39.184461
2514.769915	650955.410894	39.189479
2516.880961	652245.102470	39.194496
2519.779629	653523.583699	39.199514
2522.314868	654816.062148	39.204532
2524.852196	656110.813056	39.209549
2527.524669	657404.774200	39.214567
2529.802410	658718.952501	39.219584
2532.647614	660022.054025	39.224602
2535.329616	661328.444609	39.229620
2537.952043	662643.183709	39.234637
2540.560268	663974.025854	39.239655
2542.821867	665282.293168	39.244672
2545.832339	666595.485113	39.249690
2548.004944	667924.161248	39.254708
2550.399091	669256.994759	39.259725
2552.995697	670592.444155	39.264743
2555.233544	671935.325525	39.269760
2558.247310	673268.190326	39.274778
2560.238001	674617.246294	39.279796
2563.180595	675967.045502	39.284813
2566.233411	677311.909219	39.289831
2568.815123	678667.094792	39.294848
2571.754962	680007.462222	39.299866
2574.277344	681343.629822	39.304884
2577.013998	682681.108862	39.309901
2579.639182	684040.368735	39.314919
2582.028185	685391.965923	39.319936
2584.847324	686730.578790	39.324954
2587.560915	688084.752571	39.329972
2589.750204	689431.959284	39.334989
2592.690373	690790.010286	39.340007
2595.095634	692141.095428	39.345024
2597.705738	693490.305788	39.350042
2600.148499	694841.176003	39.355060
2602.677074	696205.618737	39.360077
2605.803531	697558.741691	39.365095
2608.179275	698922.890578	39.370112
2611.145212	700276.367611	39.375130
2613.621386	701639.186491	39.380148
2616.054956	702988.316996	39.385165
2618.775528	704353.200688	39.390183
2621.333812	705720.325198	39.395200
2624.299307	707075.325056	39.400218
2626.406467	708425.052150	39.405236
2628.841165	709765.944602	39.410253
2631.431587	711087.336763	39.415271
2633.981653	712417.741609	39.420288
2636.758043	713741.712863	39.425306
2639.439821	715066.730946	39.430324
2641.912487	716393.852906	39.435341
2644.366179	717740.563754	39.440359
2646.937391	719079.617972	39.445376
2649.438395	720418.568880	39.450394
2652.255307	721774.515524	39.455412
2654.546188	723127.707090	39.460429
2657.502267	724493.770564	39.465447
2659.783836	725850.375956	39.470464
2662.182966	727221.172309	39.475482
2664.911990	728617.335346	39.480500
2667.416280	729992.988846	39.485517
2670.150047	731375.190602	39.490535
2672.463469	732782.270664	39.495552
2675.262658	734185.273151	39.500570
2677.902887	735595.119495	39.505588
2680.172089	737008.137448	39.510605
2683.229307	738436.325698	39.515623
2685.602952	739875.426639	39.520640
2688.244383	741312.398063	39.525658
2690.752771	742762.994604	39.530676
2693.163393	744212.700370	39.535693
2695.690138	745675.584110	39.540711
2698.285994	747139.318479	39.545728
2701.176677	748613.872259	39.550746
2703.420212	750094.316842	39.555764
2706.039845	751578.951608	39.560781
2708.893377	753082.528097	39.565799
2711.453262	754586.008329	39.570816
2714.103550	756101.098800	39.575834
2717.057567	757606.435281	39.580852
2719.503278	759127.903913	39.585869
2722.384697	760653.230087	39.590887
2724.848760	762197.560202	39.595904
2727.864735	763727.462086	39.600922
2730.570496	765259.761082	39.605940
2732.910388	766801.988423	39.610957
2736.163684	768344.337751	39.615975
2738.863992	769906.811835	39.620992
2741.168953	771452.754193	39.626010
2744.601482	773011.210289	39.631028
2747.086435	774567.233685	39.636045
2749.883573	776126.757031	39.641063
2752.805513	777692.901538	39.646080
2755.545582	779252.603118	39.651098
2758.336286	780813.287638	39.656116
2760.557660	782393.704520	39.661133
2763.536271	783965.506276	39.666151
2766.265971	785556.284830	39.671168
2769.244304	787123.717242	39.676186
2772.397812	788702.496403	39.681204
2775.172303	790291.185106	39.686221
2777.845852	791853.853083	39.691239
2780.463342	793442.792863	39.696256
2783.738951	795016.961348	39.701274
2786.488568	796582.096827	39.706292
2788.967093	798174.741095	39.711309
2791.834416	799752.368975	39.716327
2794.496445	801342.398815	39.721344
2797.353124	802921.119652	39.726362
2800.433584	804517.153062	39.731380
2803.351461	806098.707869	39.736397
2806.450907	807668.181053	39.741415
2809.390949	809249.200403	39.746432
2812.162549	810782.860145	39.751450
2814.868789	812307.828134	39.756468
2817.464853	813848.642196	39.761485
2820.144092	815374.779207	39.766503
2822.468975	816920.992056	39.771520
2825.227944	818468.143822	39.776538
2827.874511	820022.326361	39.781556
2830.459522	821583.476308	39.786573
2833.063925	823142.304378	39.791591
2835.825211	824723.078965	39.796608
2838.179267	826290.619011	39.801626
2841.501456	827881.465911	39.806644
2843.914151	829484.943899	39.811661
2846.933475	831079.644105	39.816679
2849.679532	832691.195556	39.821696
2852.409770	834302.787390	39.826714
2855.078117	835920.707075	39.831732
2858.271185	837551.374880	39.836749
2861.068587	839172.008585	39.841767
2864.110381	840813.648500	39.846784
2866.517793	842471.119584	39.851802
2869.610838	844098.380767	39.856820
2872.222998	845753.695656	39.861837
2875.180271	847401.714687	39.866855
2878.298673	849064.533103	39.871872
2881.234246	850727.814765	39.876890
2884.425117	852383.617764	39.881908
2886.876954	854065.514870	39.886925
2889.889210	855740.359162	39.891943
2893.049469	857420.839528	39.896960
2895.431338	859094.682846	39.901978
2898.767736	860782.171493	39.906996
2901.832687	862475.348596	39.912013
2904.601829	864157.149139	39.917031
2907.511961	865856.681717	39.922048
2910.419679	867555.446871	39.927066
2913.435849	869262.433623	39.932084
2916.388356	870967.203104	39.937101
2919.163637	872678.002931	39.942119
2921.984342	874390.627819	39.947136
2924.753250	876106.928688	39.952154
2927.918587	877826.633188	39.957172
2930.338661	879559.594282	39.962189
2933.289886	881293.697906	39.967207
2935.941536	883025.115681	39.972224
2939.021019	884776.431911	39.977242
2942.018721	886534.768633	39.982260
2944.731990	888280.454106	39.987277
2947.999613	890029.286017	39.992295
2950.792346	891798.508480	39.997312
2953.356429	893556.998659	40.002330
2956.482061	895316.881424	40.007348
2959.144964	897100.784417	40.012365
2961.989243	898873.014821	40.017383
2965.027244	900665.276616	40.022400
2968.054372	902438.382772	40.027418
2970.938565	904225.299855	40.032436
2974.464518	906019.338098	40.037453
2977.637416	907807.085082	40.042471
2980.494530	909587.961433	40.047488
2982.931572	911373.624107	40.052506
2986.270586	913152.986016	40.057524
2988.937382	914947.163401	40.062541
2991.792835	916754.460745	40.067559
2994.581178	918564.053113	40.072576
2997.306804	920371.231124	40.077594
3000.691305	922170.501685	40.082612
3003.639478	923977.017028	40.087629
3006.344384	925751.894013	40.092647
3009.207059	927543.799910	40.097664
3012.045574	929294.377473	40.102682
3014.928312	931062.961144	40.107700
3018.032879	932845.861951	40.112717
3020.848878	934628.976827	40.117735
3023.219601	936413.573446	40.122752
3026.415053	938220.488758	40.127770
3028.856932	940013.611016	40.132788
3031.776565	941850.309742	40.137805
3034.321402	943670.460940	40.142823
3037.239609	945517.048352	40.147840
3039.906513	947372.378657	40.152858
3042.917888	949234.527638	40.157876
3045.680093	951113.890925	40.162893
3048.562921	952991.495172	40.167911
3051.820610	954874.487664	40.172928
3054.624575	956836.387082	40.177946
3057.822833	958779.463102	40.182964
3060.846699	960748.113538	40.187981
3063.840447	962725.771689	40.192999
3066.928162	964696.873648	40.198016
3069.641551	966692.558495	40.203034
3072.976133	968685.886252	40.208052
3076.252000	970679.507819	40.213069
3079.006662	972689.205132	40.218087
3082.417980	974689.410185	40.223104
3085.371080	976697.766339	40.228122
3088.618452	978725.737443	40.233140
3091.469026	980757.925627	40.238157
3094.749306	982788.735737	40.243175
3097.695239	984822.188175	40.248192
3100.678569	986858.023356	40.253210
3103.678539	988901.008007	40.258228
3106.955168	990962.371246	40.263245
3110.031296	993023.700570	40.268263
3113.337155	995069.084484	40.273280
3116.535859	997155.907885	40.278298
3119.869951	999202.127720	40.283316
3123.148708	1001267.905017	40.288333
3126.265311	1003331.499287	40.293351
3129.794840	1005401.741122	40.298368
3132.642731	1007481.517433	40.303386
3135.569984	1009551.208983	40.308404
3138.732002	1011636.767306	40.313421
3142.423957	1013699.866979	40.318439
3145.394956	1015770.461675	40.323456
3148.602844	1017861.547149	40.328474
3151.901151	1019920.298819	40.333492
3155.368670	1021994.031252	40.338509
3158.864306	1024071.245414	40.343527
3162.271452	1026127.408616	40.348544
3165.044441	1028204.270297	40.353562
3168.514950	1030275.126929	40.358580
3172.020640	1032334.204540	40.363597
3175.296042	1034402.113146	40.368615
3178.675918	1036462.002241	40.373632
3181.436435	1038523.641663	40.378650
3184.701127	1040578.939357	40.383668
3187.625566	1042643.553659	40.388685
3190.694032	1044713.155361	40.393703
3193.688946	1046777.760135	40.398720
3196.543042	1048861.445602	40.403738
3199.649247	1050951.809418	40.408756
3202.608307	1053033.713016	40.413773
3205.419254	1055124.566198	40.418791
3208.789388	1057211.844045	40.423808
3211.903839	1059299.430236	40.428826
3215.046287	1061349.632994	40.433844
3218.200291	1063399.741657	40.438861
3221.466626	1065458.950700	40.443879
3224.504967	1067496.993418	40.448896
3226.853334	1069568.528144	40.453914
3229.841375	1071624.413467	40.458932
3233.216244	1073694.697397	40.463949
3236.322940	1075786.749444	40.468967
3239.594458	1077877.781720	40.473984
3242.317339	1079984.181461	40.479002
3245.533020	1082085.189936	40.484020
3248.775915	1084202.788103	40.489037
3251.519303	1086331.306680	40.494055
3254.849972	1088477.814896	40.499072
3257.816120	1090623.248068	40.504090
3260.602623	1092772.540781	40.509108
3264.177136	1094945.284107	40.514125
3267.000630	1097123.861758	40.519143
3270.435167	1099298.218740	40.524160
3273.645165	1101498.523829	40.529178
3276.961319	1103701.725697	40.534196
3279.978302	1105906.743252	40.539213
3283.292212	1108126.708690	40.544231
3286.783954	1110339.733007	40.549248
3290.018526	1112576.621750	40.554266
3292.799473	1114813.033344	40.559284
3295.908055	1117065.472032	40.564301
3299.159959	1119326.440760	40.569319
3302.348734	1121579.911502	40.574336
3305.566059	1123861.665364	40.579354
3308.409534	1126136.717332	40.584372
3311.885674	1128436.018704	40.589389
3315.016450	1130729.454437	40.594407
3318.408294	1133037.210522	40.599424
3321.371784	1135359.853881	40.604442
3324.811799	1137681.023812	40.609460
3328.483889	1140003.126829	40.614477
3331.336005	1142335.604052	40.619495
3335.266806	1144663.471219	40.624512
3338.659856	1146987.754937	40.629530
3342.230656	1149319.677466	40.634548
3346.000400	1151639.864920	40.639565
3348.984033	1153974.073261	40.644583
3353.046303	1156300.369416	40.649600
3356.242769	1158632.285252	40.654618
3359.784701	1160972.063198	40.659636
3363.354493	1163291.664926	40.664653
3366.723896	1165617.712322	40.669671
3370.105277	1167944.700139	40.674688
3373.711373	1170278.989032	40.679706
3376.933442	1172611.638479	40.684724
3380.311742	1174949.705083	40.689741
3383.478842	1177284.783000	40.694759
3387.298849	1179612.035867	40.699776
3390.562226	1181949.322228	40.704794
3394.157291	1184275.365774	40.709812
3397.487886	1186631.175639	40.714829
3400.865297	1188982.436429	40.719847
3404.182055	1191307.709244	40.724864
3407.209765	1193654.932705	40.729882
3410.275261	1196007.355044	40.734900
3413.824138	1198370.883642	40.739917
3416.979439	1200740.874956	40.744935
3420.417924	1203097.851973	40.749952
3424.066085	1205476.890030	40.754970
3427.461115	1207841.694235	40.759988
3431.295017	1210202.626306	40.765005
3434.744409	1212547.028891	40.770010
3438.282256	1214840.135519	40.775015
3441.184353	1217090.622142	40.780020
3444.714522	1219262.265829	40.785024
3448.132976	1221355.100853	40.790029
3451.237648	1223375.325485	40.795034
3454.340558	1225309.067020	40.800039
3457.447854	1227171.536812	40.805044
3460.527641	1228956.102458	40.810048
3463.128812	1230650.799085	40.815053
3466.036048	1232275.719569	40.820058
3468.452940	1233830.782099	40.825063
3470.732714	1235287.488568	40.830068
3473.389504	1236668.654593	40.835072
3476.005071	1237986.420611	40.840077
3477.847673	1239241.421881	40.845082
3480.167682	1240408.467212	40.850087
3481.950591	1241521.742490	40.855092
3483.953194	1242559.671945	40.860096
3485.947473	1243547.449023	40.865101
3487.472025	1244474.207421	40.870106
3489.445918	1245319.563127	40.875111
3490.757132	1246126.962189	40.880116
3492.398859	1246891.333718	40.885120
3494.165402	1247572.960161	40.890125
3495.254722	1248231.099050	40.895130
3496.725319	1248827.868048	40.900135
3498.054307	1249388.919831	40.905140
3499.002359	1249903.531709	40.910144
3500.249103	1250393.895143	40.915149
3501.559143	1250822.075150	40.920154
3502.540123	1251207.002060	40.925159
3503.619933	1251559.664470	40.930164
3504.143426	1251890.111318	40.935168
3505.691164	1252177.755257	40.940173
3506.002249	1252439.685954	40.945178
3507.028981	1252674.193526	40.950183
3507.635140	1252875.156839	40.955188
3508.163818	1253041.038288	40.960192
3509.315311	1253200.407163	40.965197
3509.726888	1253317.290099	40.970202
3510.840607	1253407.602444	40.975207
3511.106238	1253503.807248	40.980212
3511.815601	1253548.426476	40.985216
3512.545180	1253561.764361	40.990221
3512.943621	1253575.527991	40.995226
3513.570723	1253561.224716	41.000231
3513.911741	1253523.579717	41.005236
3514.354533	1253494.363705	41.010240
3514.672810	1253430.641107	41.015245
3514.452520	1253358.652962	41.020250
3514.861196	1253267.254163	41.025255
3515.962796	1253173.419097	41.030260
3515.968140	1253058.970840	41.035264
3516.175702	1252941.794776	41.040269
3516.574672	1252812.424245	41.045274
3516.741593	1252654.404504	41.050279
3517.103422	1252506.373518	41.055284
3517.304293	1252335.527323	41.060288
3517.817220	1252158.496592	41.065293
3517.945814	1251983.286889	41.070298
3517.940556	1251767.426952	41.075303
3518.254736	1251573.788925	41.080308
3518.521107	1251362.602109	41.085312
3518.704823	1251138.234310	41.090317
3518.988319	1250917.461620	41.095322
3519.034276	1250672.759019	41.100327
3519.355569	1250434.314298	41.105332
3519.266180	1250197.690488	41.110336
3519.484116	1249937.506464	41.115341
3519.437878	1249679.024360	41.120346
3519.689858	1249416.671366	41.125351
3520.100076	1249154.092801	41.130356
3519.927652	1248871.158678	41.135360
3520.421297	1248601.941631	41.140365
3520.318017	1248320.265703	41.145370
3520.419629	1248030.177898	41.150375
3520.796878	1247737.054485	41.155380
3520.398593	1247434.749113	41.160384
3520.439137	1247142.947414	41.165389
3520.446140	1246840.446563	41.170394
3520.513157	1246534.385792	41.175399
3520.501691	1246228.784031	41.180404
3520.247435	1245932.406066	41.185408
3520.987302	1245617.348008	41.190413
3520.504401	1245313.999250	41.195418
3520.662470	1244990.073036	41.200423
3520.900852	1244677.641847	41.205428
3520.611544	1244355.514969	41.210432
3520.782762	1244021.482024	41.215437
3520.823870	1243720.647446	41.220442
3521.421931	1243391.059061	41.225447
3521.214123	1243064.558017	41.230452
3520.863040	1242730.339316	41.235456
3521.160761	1242400.642499	41.240461
3520.847478	1242066.745560	41.245466
3521.157911	1241728.258244	41.250471
3521.149099	1241390.824159	41.255476
3520.913156	1241057.219655	41.260480
3521.229412	1240711.219508	41.265485
3520.985755	1240377.850413	41.270490
3521.401695	1240028.716114	41.275495
3520.957757	1239695.800174	41.280500
3521.119016	1239356.898832	41.285504
3521.406705	1239007.714921	41.290509
3520.674956	1238672.079367	41.295514
3521.038006	1238326.838655	41.300519
3520.928566	1237986.120947	41.305524
3521.154768	1237639.459215	41.310528
3521.599053	1237297.114065	41.315533
3521.039470	1236940.477484	41.320538
3521.272291	1236593.277181	41.325543
3521.353660	1236258.278284	41.330548
3520.962802	1235896.976668	41.335552
3521.123779	1235537.234925	41.340557
3521.176713	1235188.384149	41.345562
3521.293061	1234835.399858	41.350567
3521.143272	1234483.180052	41.355572
3521.084792	1234127.752816	41.360576
3521.164266	1233765.196314	41.365581
3521.021736	1233421.939615	41.370586
3521.257575	1233069.184997	41.375591
3521.232438	1232705.451422	41.380596
3520.856537	1232344.731991	41.385600
3521.047131	1231991.816467	41.390605
3520.918213	1231640.700075	41.395610
3521.005696	1231289.896571	41.400615
3520.971319	1230938.529434	41.405620
3520.916394	1230578.377018	41.410624
3520.953406	1230221.260873	41.415629
3520.606185	1229870.430575	41.420634
3520.684002	1229501.880456	41.425639
3520.666697	1229142.645538	41.430644
3520.640568	1228791.874165	41.435648
3520.874687	1228425.365195	41.440653
3520.515703	1228074.692268	41.445658
3520.308908	1227721.824347	41.450663
3520.199013	1227370.688526	41.455668
3520.545846	1227025.797733	41.460672
3520.487899	1226664.994336	41.465677
3520.533955	1226309.560450	41.470682
3520.306828	1225965.905222	41.475687
3520.451464	1225610.312793	41.480692
3520.588469	1225259.083449	41.485696
3520.398578	1224893.695735	41.490701
3520.354696	1224549.541045	41.495706
3520.562978	1224184.223393	41.500711
3520.290588	1223833.242896	41.505716
3520.207806	1223476.044652	41.510720
3520.089627	1223125.363312	41.515725
3520.114039	1222775.568090	41.520730
3519.704791	1222429.088753	41.525735
3520.114812	1222077.781201	41.530740
3520.217396	1221731.263400	41.535744
3520.003090	1221368.521491	41.540749
3519.874706	1221022.834113	41.545754
3519.908620	1220659.627112	41.550759
3520.335202	1220322.488746	41.555764
3520.227283	1219955.611254	41.560768
3519.910082	1219615.278402	41.565773
3519.954770	1219255.052849	41.570778
3520.087161	1218902.637311	41.575783
3519.898853	1218567.259550	41.580788
3519.552465	1218207.024259	41.585792
3519.668213	1217852.669519	41.590797
3519.312513	1217521.924031	41.595802
3519.748856	1217168.029745	41.600807
3519.468160	1216829.654804	41.605812
3519.338598	1216483.472340	41.610816
3519.483335	1216126.748916	41.615821
3519.251649	1215794.281335	41.620826
3519.337645	1215432.656583	41.625831
3519.416249	1215089.431200	41.630836
3519.459785	1214754.512478	41.635840
3519.606730	1214402.625087	41.640845
3518.956635	1214070.675275	41.645850
3519.430279	1213718.499838	41.650855
3519.602540	1213365.227114	41.655860
3519.316617	1213027.255612	41.660864
3519.232087	1212686.140908	41.665869
3519.171389	1212345.560928	41.670874
3519.158315	1212001.862321	41.675879
3519.229084	1211654.476994	41.680884
3519.017663	1211307.020938	41.685888
3519.022094	1210968.210247	41.690893
3519.176201	1210632.628568	41.695898
3518.755134	1210275.308564	41.700903
3518.752171	1209941.485983	41.705908
3518.570955	1209611.415851	41.710912
3518.941317	1209261.290787	41.715917
3518.707556	1208934.275358	41.720922
3518.848457	1208596.783243	41.725927
3518.911569	1208254.786648	41.730932
3518.570621	1207918.733888	41.735936
3518.801444	1207576.196083	41.740941
3518.099955	1207244.935085	41.745946
3518.490266	1206913.660184	41.750951
3518.420777	1206581.502820	41.755956
3518.221291	1206251.312683	41.760960
3518.289701	1205923.212003	41.765965
3518.238986	1205588.457565	41.770970
3518.513391	1205260.374234	41.775975
3518.830098	1204917.925685	41.780980
3518.215255	1204576.451117	41.785984
3518.268759	1204238.873699	41.790989
3518.206774	1203916.945358	41.795994
3517.909217	1203579.944753	41.800999
3518.154769	1203250.425366	41.806004
3517.861924	1202933.441461	41.811008
3518.392061	1202595.771198	41.816013
3517.960873	1202264.612483	41.821018
3517.754632	1201935.833174	41.826023
3518.172831	1201608.430265	41.831028
3517.693031	1201294.001431	41.836032
3517.983870	1200952.792935	41.841037
3517.743958	1200627.592855	41.846042
3517.401452	1200315.519954	41.851047
3517.321729	1199984.812888	41.856052
3517.406240	1199680.416312	41.861056
3517.636395	1199356.559247	41.866061
3517.685356	1199027.833242	41.871066
3517.447342	1198717.428602	41.876071
3517.491548	1198389.037840	41.881076
3517.402214	1198073.221704	41.886080
3517.538431	1197750.029635	41.891085
3516.952524	1197432.473020	41.896090
3517.162930	1197122.179814	41.901095
3517.499762	1196804.526341	41.906100
3516.974281	1196483.428552	41.911104
3517.110719	1196171.025259	41.916109
3516.950255	1195862.219091	41.921114
3516.823988	1195531.045621	41.926119
3517.146539	1195223.905346	41.931124
3517.056795	1194913.622404	41.936128
3517.259648	1194593.507408	41.941133
3517.070292	1194290.527251	41.946138
3516.625706	1193963.343224	41.951143
3517.098672	1193659.277817	41.956148
3516.874682	1193355.121437	41.961152
3516.658140	1193040.989917	41.966157
3517.022854	1192728.528208	41.971162
3516.534819	1192425.957332	41.976167
3516.596756	1192115.856780	41.981172
3516.379245	1191821.190881	41.986176
3516.775793	1191496.154416	41.991181
3516.369237	1191198.383665	41.996186
3516.597056	1190892.786260	42.001191
3516.547640	1190578.007462	42.006196
3516.374824	1190284.656039	42.011200
3516.245660	1189977.183766	42.016205
3516.363398	1189670.216445	42.021210
3516.013944	1189375.902651	42.026215
3516.098711	1189073.416880	42.031220
3515.837053	1188777.926610	42.036224
3516.289899	1188469.986802	42.041229
3516.325614	1188185.224538	42.046234
3516.156957	1187868.890148	42.051239
3516.206483	1187576.288544	42.056244
3515.917505	1187284.572400	42.061248
3516.330156	1186975.045758	42.066253
3516.092426	1186679.619709	42.071258
3516.153578	1186375.945609	42.076263
3516.292907	1186074.215891	42.081268
3516.195169	1185780.314320	42.086272
3515.982843	1185469.954105	42.091277
3516.098892	1185188.776169	42.096282
3515.845565	1184870.202911	42.101287
3515.937627	1184576.295816	42.106292
3515.639779	1184286.575941	42.111296
3516.101841	1183977.426472	42.116301
3515.767262	1183697.559061	42.121306
3515.478452	1183394.802812	42.126311
3515.799079	1183098.421762	42.131316
3515.805626	1182805.839919	42.136320
3516.027773	1182496.076970	42.141325
3515.616442	1182221.601230	42.146330
3515.731170	1181910.691560	42.151335
3515.755664	1181622.652215	42.156340
3515.517669	1181323.061233	42.161344
3515.453694	1181031.991273	42.166349
3515.397997	1180753.896015	42.171354
3515.344692	1180455.165983	42.176359
3515.648284	1180176.415700	42.181364
3515.265419	1179895.786082	42.186368
3515.318534	1179592.845726	42.191373
3515.305852	1179316.643936	42.196378
3515.089604	1179035.469511	42.201383
3515.338021	1178733.011917	42.206388
3515.321771	1178454.692834	42.211392
3515.145521	1178170.168362	42.216397
3515.253596	1177876.538311	42.221402
3515.053006	1177590.290504	42.226407
3515.152452	1177299.267008	42.231412
3514.913996	1177025.901150	42.236416
3515.300139	1176740.169415	42.241421
3514.837327	1176458.330826	42.246426
3514.496500	1176182.393394	42.251431
3514.783704	1175898.045157	42.256436
3514.804711	1175611.369206	42.261440
3514.736977	1175342.033319	42.266445
3514.775039	1175065.503019	42.271450
3514.650361	1174799.352950	42.276455
3514.676804	1174518.836790	42.281460
3514.581264	1174241.907702	42.286464
3514.722949	1173954.932118	42.291469
3514.735525	1173677.106753	42.296474
3514.606811	1173407.586550	42.301479
3514.650592	1173135.478281	42.306484
3514.188993	1172859.667409	42.311488
3514.357831	1172585.529720	42.316493
3513.975140	1172318.729585	42.321498
3514.355765	1172034.154961	42.326503
3514.359859	1171762.641685	42.331508
3514.400518	1171506.387322	42.336512
3514.247280	1171234.117915	42.341517
3514.527848	1170969.308840	42.346522
3514.089268	1170690.360969	42.351527
3514.191745	1170419.610534	42.356532
3513.899323	1170163.911075	42.361536
3513.959092	1169888.517482	42.366541
3513.783823	1169631.640509	42.371546
3513.832749	1169366.788253	42.376551
3514.133971	1169104.051256	42.381556
3513.830809	1168836.493684	42.386560
3513.765156	1168577.753887	42.391565
3513.883281	1168326.803936	42.396570
3513.813000	1168056.431229	42.401575
3513.810114	1167793.206483	42.406580
3513.736516	1167528.186766	42.411584
3513.663101	1167264.852627	42.416589
3513.338070	1167007.210447	42.421594
3513.434153	1166742.878123	42.426599
3513.498829	1166490.149531	42.431604
3512.991273	1166246.377530	42.436608
3513.574134	1165983.814862	42.441613
3513.468066	1165735.609831	42.446618
3513.280691	1165478.436132	42.451623
3513.455161	1165225.533908	42.456628
3512.948665	1164981.797189	42.461632
3513.294485	1164713.638261	42.466637
3513.272633	1164470.647846	42.471642
3513.200487	1164226.332177	42.476647
3513.164194	1163959.425342	42.481652
3512.959961	1163717.657868	42.486656
3513.004282	1163460.441255	42.491661
3512.950351	1163222.876894	42.496666
3512.769353	1162987.778875	42.501671
3512.996299	1162727.662116	42.506676
3512.793013	1162488.388503	42.511680
3512.799262	1162233.574322	42.516685
3512.947863	1161989.117884	42.521690
3512.791728	1161746.117601	42.526695
3512.911540	1161505.045011	42.531700
3512.662387	1161253.816079	42.536704
3512.606551	1161011.615716	42.541709
3512.762325	1160778.536676	42.546714
3512.185043	1160532.808728	42.551719
3512.552071	1160298.917468	42.556724
3512.391710	1160067.560202	42.561728
3512.179604	1159814.176683	42.566733
3512.177278	1159591.657850	42.571738
3512.067172	1159358.086809	42.576743
3512.482848	1159111.656039	42.581748
3512.111483	1158887.277328	42.586752
3512.226464	1158643.710394	42.591757
3512.037373	1158424.481969	42.596762
3512.034339	1158198.783983	42.601767
3512.262863	1157958.192309	42.606772
3511.955055	1157736.307018	42.611776
3512.009704	1157504.990444	42.616781
3512.288983	1157269.276371	42.621786
3512.000756	1157042.913659	42.626791
3512.323675	1156813.697706	42.631796
3512.091270	1156586.171148	42.636800
3512.004746	1156346.314191	42.641805
3512.037482	1156117.777790	42.646810
3511.910411	1155881.784606	42.651815
3512.405851	1155656.462836	42.656820
3511.999256	1155429.860895	42.661824
3512.003910	1155190.882229	42.666829
3512.010914	1154967.314338	42.671834
3511.754962	1154740.468632	42.676839
3512.074377	1154510.017373	42.681844
3511.727797	1154281.463595	42.686848
3511.506037	1154055.150442	42.691853
3511.844780	1153839.902037	42.696858
3511.711159	1153621.031754	42.701863
3511.742074	1153383.480822	42.706868
3511.360322	1153171.257626	42.711872
3511.519850	1152944.266004	42.716877
3511.499225	1152723.636078	42.721882
3511.514654	1152504.316174	42.726887
3511.747522	1152277.094389	42.731892
3511.292419	1152072.317232	42.736896
3511.394828	1151844.530271	42.741901
3511.480562	1151623.363363	42.746906
3511.305247	1151399.957898	42.751911
3511.523044	1151185.757008	42.756916
3511.243585	1150968.694058	42.761920
3511.311559	1150745.978266	42.766925
3511.206141	1150536.065215	42.771930
3511.285729	1150327.154997	42.776935
3511.448667	1150111.025510	42.781940
3511.319352	1149887.927140	42.786945
3511.283318	1149675.600761	42.791949
3511.005141	1149457.907094	42.796954
3511.222173	1149234.724032	42.801959
3511.263586	1149017.906726	42.806964
3511.117515	1148809.731293	42.811969
3510.946741	1148591.226351	42.816973
3511.058912	1148393.790964	42.821978
3510.820069	1148176.037882	42.826983
3511.235535	1147962.620803	42.831988
3511.252108	1147757.598191	42.836993
3511.390030	1147538.809324	42.841997
3511.083760	1147323.779829	42.847002
3511.011516	1147112.019442	42.852007
3511.297171	1146900.002096	42.857012
3511.043495	1146693.276987	42.862017
3511.226832	1146486.471806	42.867021
3511.030988	1146267.685216	42.872026
3510.668381	1146058.204845	42.877031
3511.003142	1145838.839227	42.882036
3510.545743	1145641.489448	42.887041
3510.784492	1145429.231210	42.892045
3510.700756	1145231.615001	42.897050
3510.652580	1145021.662567	42.902055
3510.657707	1144808.469944	42.907060
3510.776518	1144610.133557	42.912065
3510.816237	1144403.080854	42.917069
3510.870080	1144196.870976	42.922074
3510.546145	1144007.307123	42.927079
3510.845201	1143798.860692	42.932084
3510.472813	1143587.198002	42.937089
3510.307914	1143389.241798	42.942093
3510.415426	1143189.052339	42.947098
3510.375856	1142984.707062	42.952103
3510.379670	1142782.338225	42.957108
3510.496618	1142603.177786	42.962113
3510.221883	1142391.735652	42.967117
3510.262239	1142201.383159	42.972122
3510.228554	1142006.767929	42.977127
3510.469821	1141802.141021	42.982132
3510.115294	1141602.347006	42.987137
3510.115540	1141405.712156	42.992141
3510.329564	1141203.438014	42.997146
3510.164754	1141015.163573	43.002151
3510.050033	1140818.051505	43.007156
3509.988853	1140628.133481	43.012161
3510.072352	1140442.738785	43.017165
3510.113371	1140246.149020	43.022170
3509.973020	1140050.910168	43.027175
3510.317715	1139859.664279	43.032180
3510.118562	1139663.566868	43.037185
3509.812571	1139470.706112	43.042189
3510.089152	1139284.859519	43.047194
3509.803112	1139096.441916	43.052199
3510.036267	1138886.768951	43.057204
3509.943818	1138706.941705	43.062209
3509.788109	1138518.292263	43.067213
3509.835870	1138324.572246	43.072218
3509.951524	1138139.850956	43.077223
3509.856266	1137943.672769	43.082228
3509.866253	1137759.430222	43.087233
3509.651007	1137576.927030	43.092237
3509.633596	1137388.404446	43.097242
3509.110241	1137196.161189	43.102247
3509.543881	1137026.822722	43.107252
3509.356678	1136839.447812	43.112257
3509.341026	1136652.512738	43.117261
3509.457005	1136478.746813	43.122266
3509.341232	1136304.823469	43.127271
3509.660195	1136119.523579	43.132276
3509.355981	1135951.126874	43.137281
3509.518123	1135764.985841	43.142285
3509.494919	1135582.952146	43.147290
3509.077535	1135410.378615	43.152295
3509.277103	1135227.061487	43.157300
3508.972819	1135058.446524	43.162305
3509.408864	1134881.536526	43.167309
3509.301067	1134700.436238	43.172314
3508.924935	1134525.547685	43.177319
3509.241952	1134344.175320	43.182324
3508.986620	1134182.838206	43.187329
3509.026358	1133996.370365	43.192333
3508.987207	1133835.557034	43.197338
3508.633448	1133649.996774	43.202343
3509.005715	1133486.635227	43.207348
3508.687917	1133322.147289	43.212353
3508.478524	1133138.635425	43.217357
3508.562154	1132979.866080	43.222362
3508.403834	1132817.426421	43.227367
3508.668780	1132651.491591	43.232372
3508.798431	1132501.821701	43.237377
3508.470573	1132328.373098	43.242381
3508.760576	1132159.473180	43.247386
3508.496639	1132002.347264	43.252391
3508.747964	1131825.651030	43.257396
3508.479424	1131666.995503	43.262401
3508.619284	1131499.239722	43.267405
3508.413208	1131343.415281	43.272410
3508.660678	1131184.660377	43.277415
3508.556604	1131014.933658	43.282420
3508.546220	1130857.637109	43.287425
3508.628946	1130689.770165	43.292429
3508.785914	1130527.493753	43.297434
3508.506408	1130364.523842	43.302439
3508.325789	1130198.585866	43.307444
3508.688898	1130040.918486	43.312449
3508.405894	1129874.416901	43.317453
3508.503785	1129712.030291	43.322458
3508.256526	1129551.882163	43.327463
3508.289566	1129394.535210	43.332468
3508.396012	1129231.942403	43.337473
3508.484002	1129065.259326	43.342477
3508.756668	1128894.166897	43.347482
3508.384662	1128745.424745	43.352487
3508.783195	1128599.499202	43.357492
3508.230768	1128434.328143	43.362497
3508.456697	1128267.977751	43.367501
3508.632668	1128101.440204	43.372506
3508.426450	1127939.620198	43.377511
3508.091953	1127784.093052	43.382516
3507.980716	1127629.475628	43.387521
3508.192938	1127473.754275	43.392525
3508.048805	1127321.225661	43.397530
3508.156954	1127161.612860	43.402535
3508.264485	1126997.049417	43.407540
3508.215827	1126846.393782	43.412545
3508.156850	1126702.869593	43.417549
3508.082077	1126544.029387	43.422554
3507.792972	1126396.920191	43.427559
3508.103850	1126238.578121	43.432564
3507.932357	1126080.405927	43.437569
3508.230677	1125928.335366	43.442573
3507.916862	1125780.071610	43.447578
3507.715108	1125636.351950	43.452583
3508.126124	1125479.683363	43.457588
3507.680606	1125327.527897	43.462593
3507.818361	1125181.932327	43.467597
3507.883557	1125030.159999	43.472602
3507.860311	1124893.336850	43.477607
3507.944649	1124742.980485	43.482612
3507.886524	1124590.645036	43.487617
3507.986125	1124441.038912	43.492621
3508.067494	1124279.155555	43.497626
3507.548345	1124137.826868	43.502631
3507.631281	1123984.689562	43.507636
3507.821269	1123844.663844	43.512641
3507.846312	1123689.624189	43.517645
3508.144437	1123552.237859	43.522650
3507.832678	1123388.107997	43.527655
3507.698397	1123230.796959	43.532660
3507.609975	1123107.359388	43.537665
3507.640697	1122950.584024	43.542669
3507.463476	1122802.405372	43.547674
3507.645008	1122654.258714	43.552679
3507.832415	1122517.815934	43.557684
3507.479588	1122379.935491	43.562689
3507.393977	1122236.866700	43.567693
3507.878450	1122093.509781	43.572698
3507.560544	1121950.471578	43.577703
3507.607161	1121789.565714	43.582708
3507.501245	1121650.768912	43.587713
3507.572760	1121519.841918	43.592717
3507.717010	1121363.096479	43.597722
3507.400239	1121224.228109	43.602727
3507.450418	1121088.342737	43.607732
3507.293278	1120950.297937	43.612737
3507.449885	1120812.769249	43.617741
3507.552668	1120678.293166	43.622746
3507.366629	1120528.434020	43.627751
3507.568195	1120384.601727	43.632756
3507.090276	1120249.829576	43.637761
3507.017532	1120106.892106	43.642765
3507.112144	1119983.161722	43.647770
3507.106299	1119852.682837	43.652775
3507.154842	1119703.904849	43.657780
3506.950510	1119565.736822	43.662785
3506.949469	1119428.960489	43.667789
3506.965328	1119304.846388	43.672794
3506.658242	1119186.307329	43.677799
3506.985660	1119045.085400	43.682804
3506.974797	1118927.444383	43.687809
3507.116554	1118783.959938	43.692813
3507.200519	1118642.672229	43.697818
3507.058707	1118515.422084	43.702823
3506.957265	1118373.776748	43.707828
3506.547060	1118252.852274	43.712833
3506.736883	1118121.250957	43.717837
3506.564622	1117995.327278	43.722842
3506.200002	1117872.385917	43.727847
3506.435475	1117743.245001	43.732852
3506.685332	1117635.155874	43.737857
3506.736269	1117517.092551	43.742861
3506.722597	1117391.604969	43.747866
3506.842845	1117270.570932	43.752871
3506.636074	1117131.196975	43.757876
3506.694311	1117009.595510	43.762881
3506.581768	1116879.538161	43.767885
3506.685499	1116745.916030	43.772890
3506.276982	1116632.578449	43.777895
3506.659480	1116511.579370	43.782900
3506.611510	1116389.981331	43.787905
3506.616971	1116279.331900	43.792909
3506.959675	1116149.944304	43.797914
3506.939785	1116013.274406	43.802919
3506.738203	1115879.776270	43.807924
3506.915987	1115756.601671	43.812929
3506.624139	1115632.643736	43.817933
3506.445840	1115509.331465	43.822938
3506.421418	1115389.994519	43.827943
3506.745722	1115260.683813	43.832948
3506.466008	1115157.588763	43.837953
3506.559009	1115023.544149	43.842957
3506.496130	1114902.296118	43.847962
3506.691098	1114793.968062	43.852967
3506.678278	1114665.556519	43.857972
3506.719778	1114548.382672	43.862977
3506.245775	1114414.892908	43.867981
3506.537218	1114292.524004	43.872986
3506.430743	1114175.843092	43.877991
3506.526928	1114047.112757	43.882996
3506.363326	1113924.429021	43.888001
3506.166266	1113806.324774	43.893005
3506.372470	1113684.242085	43.898010
3506.085889	1113584.359865	43.903015
3506.492860	1113460.618011	43.908020
3506.177970	1113344.430115	43.913025
3506.300543	1113219.871330	43.918029
3506.528490	1113107.689386	43.923034
3506.348353	1112988.801454	43.928039
3506.330803	1112856.437441	43.933044
3506.214017	1112756.034998	43.938049
3506.186868	1112645.411299	43.943053
3506.159070	1112518.762861	43.948058
3505.838063	1112416.098749	43.953063
3506.012966	1112295.324863	43.958068
3506.200690	1112182.271816	43.963073
3505.986513	1112073.097802	43.968077
3506.165154	1111952.220203	43.973082
3505.938478	1111848.575871	43.978087
3506.190973	1111735.502751	43.983092
3505.878683	1111625.191148	43.988097
3505.769244	1111520.853459	43.993101
3506.003106	1111401.671400	43.998106
3506.176539	1111299.476847	44.003111
3506.446304	1111175.609542	44.008116
3505.753628	1111075.175106	44.013121
3506.062181	1110961.217873	44.018125
3506.067224	1110841.393269	44.023130
3505.904140	1110734.282464	44.028135
3506.091390	1110628.161291	44.033140
3506.145524	1110506.890049	44.038145
3505.766086	1110400.857719	44.043149
3505.904370	1110296.646267	44.048154
3506.257108	1110188.676332	44.053159
3505.996106	1110073.267454	44.058164
3505.886723	1109970.807962	44.063169
3505.755289	1109857.281459	44.068173
3506.135989	1109745.862912	44.073178
3505.723173	1109639.057664	44.078183
3505.752188	1109526.738261	44.083188
3505.813250	1109429.965924	44.088193
3505.802688	1109322.992715	44.093197
3506.007956	1109210.828542	44.098202
3505.540144	1109100.681551	44.103207
3505.788870	1108988.410148	44.108212
3505.667268	1108889.749467	44.113217
3505.780420	1108788.948658	44.118221
3505.941014	1108685.274928	44.123226
3505.682929	1108574.605409	44.128231
3505.954929	1108470.241088	44.133236
3505.825728	1108361.836629	44.138241
3505.818559	1108262.477466	44.143245
3505.626676	1108148.638485	44.148250
3505.705037	1108044.297794	44.153255
3505.919132	1107943.941786	44.158260
3505.726133	1107841.932753	44.163265
3505.645469	1107732.266686	44.168269
3506.058221	1107635.404134	44.173274
3505.554874	1107529.717381	44.178279
3505.908146	1107410.140773	44.183284
3505.485703	1107303.863476	44.188289
3505.276729	1107220.174558	44.193293
3505.668908	1107101.825760	44.198298
3505.530155	1107009.529808	44.203303
3505.375638	1106911.029185	44.208308
3505.712248	1106812.445871	44.213313
3505.204701	1106712.472174	44.218317
3505.546129	1106606.914577	44.223322
3505.340501	1106505.073227	44.228327
3505.382408	1106402.329851	44.233332
3505.489261	1106310.745312	44.238337
3505.560515	1106215.536671	44.243341
3505.488063	1106113.379522	44.248346
3505.136723	1106026.926388	44.253351
3505.424372	1105917.162667	44.258356
3505.134844	1105823.725333	44.263361
3505.099426	1105726.615787	44.268365
3504.772172	1105625.255285	44.273370
3504.796700	1105526.604339	44.278375
3504.906310	1105441.307336	44.283380
3505.234461	1105368.292435	44.288385
3505.058661	1105275.877354	44.293389
3505.339431	1105164.762421	44.298394
3504.690844	1105084.550800	44.303399
3505.054309	1105002.834216	44.308404
3505.257538	1104914.361755	44.313409
3504.825062	1104815.773059	44.318413
3505.263023	1104726.494779	44.323418
3505.015307	1104634.462579	44.328423
3505.059608	1104536.267804	44.333428
3504.821797	1104457.029831	44.338433
3504.812680	1104367.819245	44.343437
3505.148550	1104262.503183	44.348442
3505.273458	1104184.443209	44.353447
3505.212274	1104093.994901	44.358452
3504.867103	1104007.030697	44.363457
3504.869831	1103915.900208	44.368461
3505.004102	1103813.187753	44.373466
3505.140841	1103736.170137	44.378471
3505.100959	1103640.265583	44.383476
3504.802527	1103556.725495	44.388481
3504.710286	1103462.641503	44.393485
3505.112815	1103369.811870	44.398490
3504.852661	1103275.370126	44.403495
3504.984477	1103197.963487	44.408500
3505.286451	1103108.680826	44.413505
3504.784670	1103016.662831	44.418509
3505.013341	1102933.790601	44.423514
3504.723470	1102843.167881	44.428519
3504.683147	1102757.088734	44.433524
3504.839633	1102677.950746	44.438529
3504.719805	1102594.270773	44.443533
3504.818928	1102502.622775	44.448538
3504.387715	1102423.386744	44.453543
3504.507321	1102339.950045	44.458548
3504.918698	1102258.566202	44.463553
3504.642083	1102177.294445	44.468557
3505.076481	1102095.044343	44.473562
3504.644526	1102007.775491	44.478567
3504.657012	1101921.483192	44.483572
3504.426135	1101835.994091	44.488577
3504.853486	1101759.187068	44.493581
3505.044265	1101661.775883	44.498586
3504.789667	1101587.372295	44.503591
3504.756580	1101494.582151	44.508596
3504.692548	1101404.853739	44.513601
3504.432904	1101325.668884	44.518605
3504.856591	1101240.349251	44.523610
3504.684127	1101167.742227	44.528615
3504.707149	1101078.567495	44.533620
3504.767085	1100997.891563	44.538625
3504.527316	1100918.028412	44.543629
3504.658747	1100834.662071	44.548634
3504.406851	1100757.474775	44.553639
3504.648325	1100667.301459	44.558644
3504.404545	1100596.132228	44.563649
3504.158045	1100508.808569	44.568653
3504.363236	1100438.614758	44.573658
3504.534198	1100366.322734	44.578663
3504.579880	1100288.601780	44.583668
3504.597293	1100204.001818	44.588673
3504.296845	1100123.850133	44.593677
3504.474797	1100039.985900	44.598682
3504.380078	1099978.438945	44.603687
3504.267742	1099884.391435	44.608692
3504.423009	1099814.293331	44.613697
3503.914996	1099739.905998	44.618701
3504.330072	1099666.321611	44.623706
3504.361659	1099593.277393	44.628711
3504.334054	1099525.213293	44.633716
3504.136240	1099447.520338	44.638721
3504.098512	1099365.688850	44.643725
3504.207616	1099299.798327	44.648730
3504.157954	1099240.625715	44.653735
3504.316153	1099162.487591	44.658740
3504.389627	1099087.135004	44.663745
3504.207512	1099021.958332	44.668749
3504.298189	1098932.641404	44.673754
3504.360651	1098872.012085	44.678759
3504.089571	1098790.210312	44.683764
3504.219239	1098714.747662	44.688769
3504.212634	1098647.242745	44.693773
3504.149371	1098563.873420	44.698778
3503.673045	1098499.695100	44.703783
3504.198778	1098428.179303	44.708788
3504.243588	1098356.359275	44.713793
3504.210828	1098295.452300	44.718797
3504.272176	1098231.277860	44.723802
3504.051996	1098148.884236	44.728807
3504.051996	1098077.259133	44.733812
3503.798315	1098003.762265	44.738817
3503.791673	1097941.221288	44.743821
3503.912876	1097865.174385	44.748826
3503.995907	1097815.240637	44.753831
3503.868657	1097726.130929	44.758836
3504.024371	1097678.574818	44.763841
3503.884709	1097610.887599	44.768845
3504.101000	1097528.125712	44.773850
3503.906487	1097478.138924	44.778855
3504.171228	1097403.400836	44.783860
3504.113114	1097335.122890	44.788865
3503.978557	1097266.569742	44.793869
3504.307626	1097194.113599	44.798874
3504.093421	1097131.119214	44.803879
3504.066986	1097054.415709	44.808884
3504.015926	1096997.036044	44.813889
3503.895140	1096915.468072	44.818893
3504.114793	1096847.233866	44.823898
3503.905534	1096781.652033	44.828903
3503.869065	1096699.875618	44.833908
3504.084954	1096639.961220	44.838913
3503.791640	1096575.825544	44.843917
3503.999304	1096499.266920	44.848922
3504.077764	1096440.233854	44.853927
3503.889753	1096384.974716	44.858932
3504.238362	1096313.651469	44.863937
3504.206169	1096246.981731	44.868941
3504.394282	1096174.535154	44.873946
3504.146900	1096109.812411	44.878951
3503.934407	1096022.314936	44.883956
3503.907581	1095971.712608	44.888961
3503.497499	1095906.918566	44.893965
3504.041493	1095830.295086	44.898970
3503.899521	1095765.455191	44.903975
3503.918015	1095699.822725	44.908980
3503.678839	1095631.170403	44.913985
3503.885365	1095578.899546	44.918989
3503.894679	1095516.710591	44.923994
3503.756581	1095454.832225	44.928999
3503.872061	1095391.380569	44.934004
3504.271396	1095316.782850	44.939009
3503.730627	1095265.875856	44.944013
3504.129430	1095187.832028	44.949018
3503.745833	1095123.789675	44.954023
3503.426995	1095069.878177	44.959028
3503.601940	1094998.087796	44.964033
3503.274562	1094938.148354	44.969037
3503.796358	1094877.494279	44.974042
3503.528023	1094816.395542	44.979047
3503.592119	1094745.768308	44.984052
3503.698187	1094694.940778	44.989057
3503.506184	1094645.405824	44.994061
3503.524563	1094565.884662	44.999066
3503.397128	1094522.844915	45.004071
3503.701952	1094461.934851	45.009076
3503.792964	1094411.681297	45.014081
3503.639654	1094350.941133	45.019085
3503.873652	1094271.762918	45.024090
3503.747980	1094220.490624	45.029095
3503.673817	1094162.797610	45.034100
3503.985952	1094103.891972	45.039105
3503.830327	1094037.502437	45.044109
3504.026773	1093971.724010	45.049114
3503.854155	1093919.308181	45.054119
3503.552356	1093835.331022	45.059124
3503.851336	1093779.677949	45.064129
3503.825252	1093722.068026	45.069133
3503.882565	1093659.754128	45.074138
3503.794021	1093591.146817	45.079143
3503.674203	1093514.982760	45.084148
3504.035054	1093452.903619	45.089153
3503.635985	1093405.114202	45.094157
3503.583624	1093334.009182	45.099162
3503.784366	1093275.782879	45.104167
3503.586007	1093225.087410	45.109172
3503.390044	1093153.429384	45.114177
3503.491926	1093100.768988	45.119181
3503.695755	1093042.443953	45.124186
3503.553950	1092982.260844	45.129191
3503.882677	1092923.722525	45.134196
3504.153833	1092857.248229	45.139201
3503.483901	1092804.520630	45.144205
3503.723230	1092740.156020	45.149210
3503.553216	1092685.430464	45.154215
3503.915069	1092620.852811	45.159220
3503.635617	1092559.921879	45.164225
3503.450026	1092505.579977	45.169229
3503.548622	1092444.489755	45.174234
3503.654357	1092384.354962	45.179239
3503.106602	1092324.422862	45.184244
3503.270617	1092262.649704	45.189249
3503.374314	1092220.319436	45.194253
3503.407441	1092155.407453	45.199258
3503.512777	1092108.959512	45.204263
3503.259408	1092050.699110	45.209268
3503.757469	1091992.314320	45.214273
3503.458789	1091940.570251	45.219277
3503.495056	1091880.058358	45.224282
3503.349353	1091821.203326	45.229287
3503.422164	1091768.439036	45.234292
3503.485384	1091709.931347	45.239297
3503.012851	1091655.723920	45.244301
3503.026644	1091590.999847	45.249306
3503.203685	1091552.003294	45.254311
3503.233824	1091504.700868	45.259316
3503.404562	1091447.130083	45.264321
3503.488600	1091398.285919	45.269325
3503.134779	1091347.023995	45.274330
3503.378768	1091296.524861	45.279335
3503.340980	1091246.837662	45.284340
3503.418952	1091182.002389	45.289345
3503.074229	1091136.577750	45.294349
3503.342446	1091077.167709	45.299354
3503.347278	1091033.216669	45.304359
3503.007046	1090973.139676	45.309364
3503.050322	1090931.766844	45.314369
3503.126172	1090878.323109	45.319373
3503.208402	1090826.984446	45.324378
3503.216253	1090781.403004	45.329383
3503.011640	1090735.281620	45.334388
3503.328692	1090678.731926	45.339393
3503.161016	1090623.410602	45.344397
3503.378440	1090579.803915	45.349402
3503.265859	1090523.419125	45.354407
3502.844467	1090476.756673	45.359412
3503.138940	1090432.178481	45.364417
3503.240188	1090387.344454	45.369421
3503.160115	1090326.834391	45.374426
3503.331821	1090280.551394	45.379431
3503.380610	1090234.096713	45.384436
3503.491625	1090176.426515	45.389441
3503.073477	1090117.980935	45.394445
3502.775856	1090076.083107	45.399450
3503.173620	1090028.707261	45.404455
3503.038997	1089975.959699	45.409460
3503.186897	1089925.846727	45.414465
3503.069018	1089884.683998	45.419469
3503.178338	1089832.852601	45.424474
3503.201261	1089789.942025	45.429479
3503.249722	1089743.004319	45.434484
3503.573568	1089693.817987	45.439489
3503.114134	1089641.024887	45.444493
3503.312220	1089595.976820	45.449498
3503.419114	1089534.086222	45.454503
3503.109540	1089489.695562	45.459508
3503.324989	1089436.980883	45.464513
3502.969021	1089393.554889	45.469517
3503.173030	1089327.431529	45.474522
3503.401790	1089284.961976	45.479527
3502.964649	1089238.291452	45.484532
3503.398686	1089183.047903	45.489537
3503.108289	1089139.034355	45.494541
3502.966917	1089076.892075	45.499546
3502.984616	1089044.513095	45.504551
3502.939932	1088989.250633	45.509556
3503.175561	1088941.604646	45.514561
3503.223351	1088898.299766	45.519565
3502.922699	1088845.951725	45.524570
3503.017846	1088805.128886	45.529575
3503.216740	1088752.314497	45.534580
3503.116444	1088707.403997	45.539585
3502.957695	1088665.376599	45.544589
3503.037830	1088618.519749	45.549594
3503.136022	1088576.353548	45.554599
3502.813617	1088526.879904	45.559604
3503.512164	1088480.303198	45.564609
3502.924169	1088430.010230	45.569613
3503.042688	1088381.899628	45.574618
3503.172661	1088329.188278	45.579623
3502.919872	1088276.922663	45.584628
3503.464794	1088231.901962	45.589633
3503.100460	1088191.341792	45.594637
3502.867950	1088143.670108	45.599642
3503.018734	1088095.072632	45.604647
3503.302297	1088045.111572	45.609652
3503.208917	1088001.822794	45.614657
3502.769441	1087957.057755	45.619661
3502.827670	1087897.934938	45.624666
3503.399429	1087859.996559	45.629671
3503.090328	1087826.993479	45.634676
3503.584169	1087767.797502	45.639681
3503.210469	1087708.073083	45.644685
3503.312197	1087651.718963	45.649690
3503.390694	1087607.344792	45.654695
3503.121000	1087561.398762	45.659700
3503.286327	1087508.098737	45.664705
3503.274114	1087464.792310	45.669709
3502.743436	1087400.587003	45.674714
3502.892471	1087366.739131	45.679719
3503.039743	1087318.231105	45.684724
3503.035482	1087265.819002	45.689729
3503.132794	1087234.470134	45.694733
3503.180119	1087174.862144	45.699738
3503.158512	1087136.633168	45.704743
3503.042833	1087095.736385	45.709748
3502.919137	1087037.879866	45.714753
3502.897278	1087000.033264	45.719757
3503.126095	1086950.933585	45.724762
3502.944410	1086903.434288	45.729767
3503.072067	1086855.212839	45.734772
3502.556911	1086811.313249	45.739777
3502.840470	1086773.127282	45.744781
3502.701892	1086724.086064	45.749786
3503.018918	1086689.152185	45.754791
3502.729422	1086653.263843	45.759796
3502.944870	1086588.446889	45.764801
3502.603416	1086563.587123	45.769805
3502.827102	1086528.475922	45.774810
3502.850341	1086467.426652	45.779815
3503.021262	1086355.943073	45.784820
3502.708101	1086182.913024	45.789825
3502.709231	1085958.166769	45.794829
3502.410046	1085670.105721	45.799834
3502.565162	1085339.587489	45.804839
3502.630456	1084935.539341	45.809844
3502.668460	1084468.192579	45.814849
3502.474717	1083938.619231	45.819853
3502.419489	1083340.123833	45.824858
3502.096010	1082671.599865	45.829863
3502.400630	1081940.259256	45.834868
3502.171945	1081137.922380	45.839873
3501.617493	1080269.320853	45.844877
3501.723517	1079335.604032	45.849882
3501.803128	1078324.182792	45.854887
3501.097004	1077253.090348	45.859892
3501.093345	1076100.346917	45.864897
3500.823951	1074875.088050	45.869901
3500.496642	1073571.467283	45.874906
3500.680253	1072184.050446	45.879911
3500.095237	1070746.719674	45.884916
3500.368569	1069208.984564	45.889921
3499.640317	1067600.878773	45.894925
3499.722591	1065900.398379	45.899930
3499.102177	1064135.805495	45.904935
3498.818013	1062280.974223	45.909940
3498.558826	1060349.731366	45.914945
3498.247466	1058338.638516	45.919949
3497.878423	1056234.793565	45.924954
3497.796591	1054057.122233	45.929959
3497.617548	1051812.256123	45.934964
3497.396489	1049464.310592	45.939969
3496.528620	1047037.000532	45.944973
3496.541571	1044533.351309	45.949978
3495.843450	1041943.089375	45.954983
3495.159611	1039273.031937	45.959988
3494.871106	1036531.416904	45.964993
3494.474655	1033700.323814	45.969997
3493.644451	1030784.609584	45.975002
3493.240046	1027799.887523	45.980007
3492.746303	1024733.148724	45.985012
3492.409398	1021581.505865	45.990017
3491.733676	1018356.737576	45.995021
3491.383577	1015030.652983	46.000026
3490.419018	1011639.463948	46.005031
3489.919010	1008165.966715	46.010036
3489.459432	1004609.694711	46.015041
3488.526231	1000971.457060	46.020045
3488.140530	997254.341049	46.025050
3487.658847	993455.184773	46.030055
3486.916262	989583.608391	46.035060
3486.190059	985604.586458	46.040065
3486.007563	981574.942144	46.045069
3484.757007	977444.219450	46.050074
3484.126170	973242.832482	46.055079
3483.228742	968957.763250	46.060084
3482.485211	964582.788782	46.065089
3481.436693	960134.942081	46.070093
3480.860694	955613.543258	46.075098
3479.940847	951097.127689	46.080103
3478.989705	946528.227298	46.085108
3478.209858	941877.705924	46.090113
3477.042090	937155.838776	46.095117
3476.387627	932341.391548	46.100122
3475.405329	927457.074626	46.105127
3474.163956	922495.803638	46.110132
3473.450535	917442.935691	46.115137
3472.397170	912335.325191	46.120141
3471.297848	907124.294320	46.125146
3470.313462	901860.181381	46.130151
3469.333459	896487.621468	46.135156
3468.332967	891045.940324	46.140161
3467.193106	885521.172239	46.145165
3466.096899	879915.729226	46.150170
3464.896817	874228.013522	46.155175
3463.513522	868477.293348	46.160180
3462.624041	862630.388358	46.165185
3461.391710	856715.353477	46.170189
3460.064709	850717.219308	46.175194
3459.076953	844636.530388	46.180199
3457.498588	838485.186504	46.185204
3456.452109	832240.362285	46.190209
3455.399900	825917.849615	46.195213
3453.941076	819522.029939	46.200218
3452.714662	813051.646612	46.205223
3450.974159	806485.321052	46.210228
3450.156721	799843.248268	46.215233
3448.574221	793126.225333	46.220237
3447.101575	786328.928320	46.225242
3445.756265	779449.357755	46.230247
3443.919772	772516.703264	46.235252
3443.205460	765473.600385	46.240257
3441.188892	758374.446952	46.245261
3439.848166	751188.883934	46.250266
3438.555324	743928.759932	46.255271
3436.672359	736592.856200	46.260276
3435.062718	729151.416845	46.265281
3433.329544	721658.446319	46.270285
3431.725823	714074.483957	46.275290
3430.193349	706428.935541	46.280295
3428.305443	698704.837965	46.285300
3426.561765	690896.764643	46.290305
3424.988010	683044.778869	46.295309
3423.333300	675089.879675	46.300314
3421.642067	667058.137834	46.305319
3419.748236	658976.602185	46.310324
3417.771380	650798.305249	46.315329
3415.784285	642557.915289	46.320333
3414.174140	634250.772918	46.325338
3412.218801	625872.341878	46.330343
3410.105697	617428.204662	46.335348
3408.206462	608911.443379	46.340353
3406.086957	600319.274749	46.345357
3404.202143	591670.574174	46.350362
3402.244203	582949.054667	46.355367
3399.892532	574152.328645	46.360372
3398.027213	565288.133071	46.365377
3395.482946	556375.352999	46.370381
3393.356776	547389.194698	46.375386
3391.589491	538337.740268	46.380391
3389.066098	529231.746772	46.385396
3386.845953	520048.861197	46.390401
3384.485401	510813.684875	46.395405
3382.385180	501511.145248	46.400410
3379.940739	492155.251360	46.405415
3377.283801	482739.271645	46.410420
3375.250908	473241.407628	46.415425
3372.511588	463715.591238	46.420429
3369.952756	454125.655368	46.425434
3367.397547	444475.060952	46.430439
3364.867217	434785.416966	46.435444
3362.098117	425016.942367	46.440449
3359.174087	415212.880197	46.445453
3356.604455	405350.860868	46.450458
3353.958428	395442.516861	46.455463
3350.846081	385499.953495	46.460468
3348.313183	375499.436356	46.465473
3345.196755	365461.421629	46.470477
3342.302865	355365.669814	46.475482
3339.268776	345243.445199	46.480487
3336.104860	335085.261895	46.485492
3332.910355	324873.775980	46.490497
3329.516817	314642.269524	46.495501
3326.180569	304382.755319	46.500506
3322.833212	294082.028077	46.505511
3318.767565	283754.288149	46.510516
3315.795320	273412.769312	46.515521
3312.285890	263042.625933	46.520525
3308.768968	252645.391376	46.525530
3304.976461	242215.782211	46.530535
3301.188916	231789.786596	46.535540
3297.766460	221247.866620	46.540545
3293.598742	210785.728693	46.545549
3289.373912	200318.880689	46.550554
3285.533176	189838.255437	46.555559
3280.928893	179367.972590	46.560564
3276.793031	168879.253890	46.565569
3272.191202	158408.223581	46.570573
3267.402075	147948.456341	46.575578
3262.246194	137503.268011	46.580583
3257.034159	127082.902333	46.585588
3251.919086	116672.374153	46.590593
3246.721924	106327.914905	46.595597
3240.460512	96006.640391	46.600602
3234.857985	85722.869733	46.605607
3228.345656	75505.872643	46.610612
3221.619272	65337.253066	46.615617
3214.232214	55278.819736	46.620621
3205.764542	45309.025438	46.625626
3196.342351	35485.942278	46.630631
3177.258185	26019.466860	46.635636
3147.982300	17059.055823	46.640641
3117.209720	8523.230362	46.645645
3051.021702	1488.664638	46.650650
2801.660800	382.270223	46.655655
2608.270645	393.091407	46.660660
2544.326995	390.522211	46.665665
2582.718730	385.287891	46.670669
2671.707579	380.547281	46.675674
2764.130321	352.176384	46.680679
2829.948263	345.622314	46.685684
2862.664336	335.837862	46.690689
2867.574086	341.753575	46.695693
2857.027492	355.927580	46.700698
2843.105195	340.124991	46.705703
2830.082331	339.029598	46.710708
2821.643384	329.859213	46.715713
2817.199843	333.279702	46.720717
2815.031885	336.568520	46.725722
2814.485144	336.771773	46.730727
2812.801343	333.582163	46.735732
2811.873760	333.154929	46.740737
2809.943324	322.311496	46.745741
2807.021900	322.736067	46.750746
2803.859815	324.196274	46.755751
2800.278645	330.308860	46.760756
2797.199119	322.763810	46.765761
2794.361603	319.242218	46.770765
2791.552582	311.247191	46.775770
2788.135136	307.468315	46.780775
2785.036790	310.874910	46.785780
2781.610559	312.141796	46.790785
2778.658580	308.054631	46.795789
2775.373998	314.340601	46.800794
2772.650242	307.438377	46.805799
2769.137336	311.804509	46.810804
2765.938853	301.833354	46.815809
2762.749419	309.396460	46.820813
2759.049458	312.592269	46.825818
2756.208406	295.968551	46.830823
2752.475068	306.751962	46.835828
2749.562977	301.988738	46.840833
2746.129608	297.175906	46.845837
2742.774610	303.064948	46.850842
2739.661456	299.506646	46.855847
2736.485569	295.969048	46.860852
2732.703977	284.531116	46.865857
2729.307406	286.578156	46.870861
2725.700095	292.535340	46.875866
2722.560980	290.270299	46.880871
2718.895077	297.727087	46.885876
2715.923625	285.824789	46.890881
2712.702281	283.277829	46.895885
2708.940194	289.896983	46.900890
2705.843919	280.908726	46.905895
2702.196640	284.158321	46.910900
2699.174138	285.417473	46.915905
2695.572290	281.847920	46.920909
2692.103451	288.111212	46.925914
2688.897944	283.756107	46.930919
2685.164827	293.431170	46.935924
2681.904110	288.698725	46.940929
2678.560472	287.353081	46.945933
2674.445134	289.462124	46.950938
2671.693704	283.836814	46.955943
2668.006031	281.299381	46.960948
2664.783786	280.043534	46.965953
2661.553464	278.779254	46.970957
2657.945013	281.420947	46.975962
2654.661644	279.107110	46.980967
2650.788362	276.512484	46.985972
2647.186846	278.040075	46.990977
2644.549341	277.537762	46.995981
2641.281076	271.342106	47.000986
2637.254902	272.259572	47.005991
2633.402170	283.833809	47.010996
2630.348734	274.730400	47.016001
2627.114295	274.585498	47.021005
2623.405655	281.764438	47.026010
2620.274264	272.127422	47.031015
2616.389230	279.152636	47.036020
2612.766748	280.343822	47.041025
2609.279305	277.091380	47.046029
2606.124595	279.622168	47.051034
2602.623845	270.848551	47.056039
2598.672456	276.053225	47.061044
2595.577051	267.163841	47.066049
2592.318604	266.906595	47.071053
2588.745959	267.634860	47.076058
2585.883309	268.774563	47.081063
2582.160479	272.884533	47.086068
2578.417881	261.407331	47.091073
2574.565419	260.668428	47.096077
2571.231261	268.487585	47.101082
2568.298851	258.081015	47.106087
2564.822145	255.523552	47.111092
2560.791639	251.345104	47.116097
2557.378725	265.193805	47.121101
2554.230880	269.488964	47.126106
2550.755958	252.053398	47.131111
2546.640013	264.772967	47.136116
2543.444450	255.951928	47.141121
2540.736324	254.219590	47.146125
2536.789242	262.221910	47.151130
2533.814865	247.468511	47.156135
2529.456847	264.130022	47.161140
2526.216191	250.224597	47.166145
2523.021923	256.742289	47.171149
2519.222206	259.167257	47.176154
2515.822228	245.304295	47.181159
2512.527130	257.667322	47.186164
2509.006036	250.156295	47.191169
2505.492400	254.948942	47.196173
2501.737696	260.297621	47.201178
2498.493972	247.708915	47.206183
2494.959522	253.696291	47.211188
2491.699192	250.479369	47.216193
2488.036568	249.392020	47.221197
2484.083945	248.647286	47.226202
2481.149764	242.483052	47.231207
2477.533029	251.187325	47.236212
2473.969835	241.108591	47.241217
2470.976604	244.912515	47.246221
2467.035490	244.529643	47.251226
2463.698487	231.722436	47.256231
2460.273132	253.365190	47.261236
2456.600464	238.194049	47.266241
2453.329158	247.746450	47.271245
2449.691714	245.768232	47.276250
2446.488332	237.581334	47.281255
2442.688062	249.084122	47.286260
2439.116731	239.528553	47.291265
2435.976056	243.790898	47.296269
2432.452061	241.781451	47.301274
2429.059226	232.667348	47.306279
2425.035500	244.139607	47.311284
2421.458931	231.766365	47.316289
2418.088127	235.100315	47.321293
2414.941688	232.017866	47.326298
2411.596854	230.202541	47.331303
2407.861862	234.102866	47.336308
2404.196258	241.042936	47.341313
2400.916518	231.291516	47.346317
2397.049930	240.004659	47.351322
2394.091523	229.663356	47.356327
2390.452574	245.707994	47.361332
2386.914489	233.692472	47.366337
2383.481403	236.830908	47.371341
2379.877497	230.624356	47.376346
2376.507990	223.397607	47.381351
2372.914536	235.979161	47.386356
2369.308639	225.725715	47.391361
2365.924439	234.164168	47.396365
2362.259000	231.315422	47.401370
2359.111279	237.417538	47.406375
2355.134044	231.968599	47.411380
2351.869431	231.365595	47.416385
2348.085563	231.586091	47.421389
2344.857987	231.980132	47.426394
2341.958872	223.013936	47.431399
2338.158185	232.662751	47.436404
2334.468806	234.433661	47.441409
2331.387672	224.159299	47.446413
2327.471283	233.400705	47.451418
2324.071367	222.739009	47.456423
2320.321353	227.814888	47.461428
2316.935795	229.034418	47.466433
2313.815433	221.631155	47.471437
2309.790652	242.631874	47.476442
2306.713195	220.597831	47.481447
2302.921403	226.428036	47.486452
2299.382153	220.940046	47.491457
2296.428404	222.629009	47.496461
2292.689765	229.681204	47.501466
2289.210070	221.441903	47.506471
2285.254026	230.083319	47.511476
2282.050370	226.794210	47.516481
2278.605428	227.154182	47.521485
2275.136132	232.048424	47.526490
2271.777209	226.686483	47.531495
2268.097169	227.614928	47.536500
2264.274488	226.220235	47.541505
2261.170233	229.493119	47.546509
2257.763925	233.332888	47.551514
2254.015754	224.507465	47.556519
2250.441840	236.191805	47.561524
2247.327914	221.764090	47.566529
2243.575347	226.877124	47.571533
2239.860766	225.213532	47.576538
2236.747470	219.729904	47.581543
2233.075430	225.279340	47.586548
2229.316641	228.190585	47.591553
2226.257120	216.437001	47.596557
2222.740136	222.783767	47.601562
2219.888069	214.505706	47.606567
2215.718556	230.923904	47.611572
2212.117226	219.704341	47.616577
2208.582408	216.978173	47.621581
2204.937946	226.165007	47.626586
2201.704395	218.219309	47.631591
2197.844773	224.842607	47.636596
2194.614993	224.882896	47.641601
2191.082445	213.796341	47.646605
2187.751826	221.724045	47.651610
2184.322132	212.286655	47.656615
2180.828018	222.798032	47.661620
2177.249977	224.885790	47.666625
2173.356238	219.319995	47.671629
2169.778014	221.335273	47.676634
2166.662533	219.757585	47.681639
2163.343729	215.821985	47.686644
2159.505637	216.950978	47.691649
2156.458586	218.778607	47.696653
2152.826541	221.327430	47.701658
2149.343729	215.198510	47.706663
2145.934353	215.280875	47.711668
2142.413939	212.770399	47.716673
2138.935594	217.803319	47.721677
2134.603370	210.760961	47.726682
2131.623866	213.347180	47.731687
2128.167742	208.393319	47.736692
2124.643214	217.637941	47.741697
2121.570087	206.898987	47.746701
2117.443120	217.412074	47.751706
2114.557204	210.650287	47.756711
2110.557580	209.178514	47.761716
2107.160179	211.319081	47.766721
2103.866004	212.999158	47.771725
2100.181714	208.791899	47.776730
2096.724722	207.532710	47.781735
2093.385228	210.103939	47.786740
2089.854617	208.371800	47.791745
2086.450349	211.702920	47.796749
2082.862574	208.840823	47.801754
2079.254722	205.206596	47.806759
2075.556262	207.196368	47.811764
2071.695777	207.834236	47.816769
2068.352269	215.954121	47.821773
2065.018993	214.321247	47.826778
2061.947741	208.665027	47.831783
2058.438140	203.091186	47.836788
2054.732896	204.747245	47.841793
2051.115884	202.194642	47.846797
2047.561973	204.964736	47.851802
2044.124814	205.013157	47.856807
2040.699980	202.853872	47.861812
2036.998592	209.672619	47.866817
2034.176335	197.080793	47.871821
2030.013585	201.197863	47.876826
2026.837220	204.301396	47.881831
2023.513619	210.763829	47.886836
2019.404717	205.359708	47.891841
2016.616446	208.089539	47.896845
2012.566734	207.206680	47.901850
2009.466437	192.511003	47.906855
2005.664753	199.905196	47.911860
2002.059304	198.013983	47.916865
1998.458551	196.632745	47.921869
1995.235002	202.774520	47.926874
1991.682287	201.189723	47.931879
1988.462296	196.340431	47.936884
1984.677542	197.768425	47.941889
1981.174361	191.351632	47.946893
1977.629555	197.952089	47.951898
1974.134846	190.579101	47.956903
1971.084304	194.173434	47.961908
1966.911411	197.254338	47.966913
1964.155367	199.143936	47.971917
1959.964115	201.185071	47.976922
1956.770546	196.614679	47.981927
1953.410936	194.121380	47.986932
1949.745768	202.798702	47.991937
1946.350048	190.584780	47.996941
1942.949368	199.029442	48.001946
1939.193084	197.011412	48.006951
1935.634034	197.322296	48.011956
1932.032305	204.063181	48.016961
1928.674264	196.035475	48.021965
1924.990766	202.484707	48.026970
1921.744384	200.597831	48.031975
1917.842007	197.588933	48.036980
1914.525359	200.819146	48.041985
1911.679610	195.833861	48.046989
1907.702812	202.656663	48.051994
1904.234148	200.483070	48.056999
1900.814689	199.431871	48.062004
1896.933148	208.482915	48.067009
1893.983528	204.606903	48.072013
1890.159439	196.602835	48.077018
1886.978437	200.549718	48.082023
1883.092797	197.147398	48.087028
1879.845904	198.827563	48.092033
1876.338077	193.456173	48.097037
1872.614607	199.103134	48.102042
1869.367534	204.224091	48.107047
1865.707817	192.060678	48.112052
1862.173501	193.590762	48.117057
1858.734392	193.972264	48.122061
1854.842114	185.881902	48.127066
1851.680198	186.769559	48.132071
1848.146230	196.478236	48.137076
1844.737426	191.135809	48.142081
1841.455838	188.340530	48.147085
1837.431550	198.340448	48.152090
1834.010921	193.136518	48.157095
1831.002153	188.845285	48.162100
1827.182190	195.955382	48.167105
1823.946216	185.006697	48.172109
1819.811837	205.266049	48.177114
1816.488429	190.054920	48.182119
1813.151165	188.976291	48.187124
1809.252957	200.780077	48.192129
1806.458022	193.678259	48.197133
1802.591462	194.887703	48.202138
1799.343724	189.269025	48.207143
1795.755688	188.404431	48.212148
1792.363835	198.626474	48.217153
1788.784794	190.284786	48.222157
1784.931646	202.031819	48.227162
1781.409295	188.095233	48.232167
1778.406915	192.658590	48.237172
1774.896580	194.275720	48.242177
1771.598877	184.278238	48.247181
1767.213798	196.320815	48.252186
1763.732567	193.767468	48.257191
1760.489443	187.361954	48.262196
1757.078087	186.586319	48.267201
1753.609985	188.709899	48.272205
1750.231386	186.635869	48.277210
1746.540081	187.208305	48.282215
1743.137020	192.367576	48.287220
1739.242258	191.532016	48.292225
1736.419231	184.259163	48.297229
1732.726791	190.262149	48.302234
1729.416968	186.313749	48.307239
1725.440858	184.939144	48.312244
1721.729026	183.068297	48.317249
1718.740858	179.370198	48.322253
1715.159040	193.295213	48.327258
1711.477903	179.379160	48.332263
1708.271080	186.493695	48.337268
1704.643161	188.221814	48.342273
1701.229008	189.254747	48.347277
1697.357186	189.973706	48.352282
1694.268635	186.093782	48.357287
1690.341166	184.682067	48.362292
1686.942076	193.737542	48.367297
1683.741865	186.482262	48.372301
1680.014401	189.404976	48.377306
1677.050808	183.032108	48.382311
1673.210804	192.254167	48.387316
1669.536109	189.296436	48.392321
1666.515984	183.334336	48.397325
1662.367970	179.325494	48.402330
1658.860457	178.851386	48.407335
1655.688298	178.651157	48.412340
1651.737831	183.934142	48.417345
1648.735585	184.201428	48.422349
1645.235721	181.729257	48.427354
1641.252531	183.367358	48.432359
1637.873040	187.242912	48.437364
1634.433719	188.586851	48.442369
1631.111031	183.727065	48.447373
1627.345769	180.004525	48.452378
1624.052292	179.581142	48.457383
1620.471373	172.240743	48.462388
1617.155012	187.966166	48.467393
1614.059661	178.317975	48.472397
1610.336746	177.207291	48.477402
1606.336069	188.628998	48.482407
1603.141896	181.124547	48.487412
1599.043915	175.397873	48.492417
1595.833041	177.462600	48.497421
1592.471560	178.572131	48.502426
1589.226864	177.800448	48.507431
1585.724579	173.350156	48.512436
1581.942053	174.039840	48.517441
1578.692923	178.093387	48.522445
1574.739797	177.167712	48.527450
1571.407827	178.265180	48.532455
1567.889610	170.411516	48.537460
1564.647474	185.133699	48.542465
1561.285000	166.160923	48.547469
1557.676023	178.228721	48.552474
1553.908251	174.138256	48.557479
1550.473473	176.403526	48.562484
1547.074182	177.289251	48.567489
1543.542804	181.784907	48.572493
1539.992909	179.890986	48.577498
1536.349884	177.102332	48.582503
1532.765817	174.590054	48.587508
1529.425740	183.450962	48.592513
1526.151183	168.153249	48.597517
1522.381100	173.433854	48.602522
1518.928817	167.128009	48.607527
1515.597091	170.252157	48.612532
1512.141061	172.359156	48.617537
1508.624933	171.464692	48.622541
1504.928849	176.663737	48.627546
1501.236595	173.091018	48.632551
1497.875464	169.871992	48.637556
1494.089959	169.381496	48.642561
1491.006169	172.882743	48.647565
1487.619008	176.865287	48.652570
1483.901108	164.422487	48.657575
1480.566823	173.325072	48.662580
1477.009151	175.450047	48.667585
1473.427504	174.271727	48.672589
1469.975343	170.202918	48.677594
1466.061640	180.227364	48.682599
1462.926985	168.836967	48.687604
1459.452571	168.847325	48.692609
1456.588675	163.242929	48.697613
1452.527803	161.809075	48.702618
1449.012021	164.157806	48.707623
1445.880253	169.672767	48.712628
1442.097277	163.208450	48.717633
1438.248666	169.161571	48.722637
1434.412069	178.791208	48.727642
1430.927239	174.702752	48.732647
1427.952740	167.744612	48.737652
1423.972022	168.156620	48.742657
1420.776979	172.662129	48.747661
1416.941117	163.730384	48.752666
1413.857350	165.279351	48.757671
1410.805654	163.557509	48.762676
1406.823491	173.941928	48.767681
1404.010460	164.764320	48.772685
1399.827302	173.840193	48.777690
1396.007178	176.783175	48.782695
1392.937020	170.097050	48.787700
1389.423547	180.692591	48.792705
1385.937638	166.787757	48.797709
1382.127318	180.657465	48.802714
1378.826545	170.180171	48.807719
1375.333823	167.874780	48.812724
1371.725614	176.764513	48.817729
1368.380815	162.920063	48.822733
1364.533360	165.911965	48.827738
1361.262381	160.882689	48.832743
1357.899433	157.514575	48.837748
1354.345744	173.168248	48.842753
1350.863487	160.035810	48.847757
1347.340270	170.284320	48.852762
1343.656362	164.682242	48.857767
1340.705535	161.774314	48.862772
1336.894862	160.631109	48.867777
1333.610697	166.435173	48.872781
1329.663578	165.843784	48.877786
1326.430131	170.381813	48.882791
1322.837557	170.875526	48.887796
1319.069097	167.549404	48.892801
1315.660367	160.292152	48.897805
1312.362803	165.483711	48.902810
1308.712538	154.282310	48.907815
1305.474119	162.012687	48.912820
1301.615221	163.805671	48.917825
1298.629011	165.226214	48.922829
1294.947291	170.705439	48.927834
1291.095036	170.747273	48.932839
1287.830213	167.431857	48.937844
1284.372991	169.973641	48.942849
1281.048364	170.500984	48.947853
1277.091096	173.428584	48.952858
1273.533778	165.472930	48.957863
1270.189985	168.857067	48.962868
1266.595264	165.691716	48.967873
1263.352782	164.705740	48.972877
1259.387446	163.783152	48.977882
1256.195337	167.093223	48.982887
1253.181097	159.963266	48.987892
1249.300935	160.739982	48.992897
1245.851872	161.460235	48.997901
1242.174694	156.945975	49.002906
1238.738781	170.631396	49.007911
1235.095207	158.889879	49.012916
1231.508582	159.656328	49.017921
1228.525753	167.057554	49.022925
1224.840433	169.946801	49.027930
1221.129169	164.852063	49.032935
1217.607882	156.545500	49.037940
1214.001637	170.747887	49.042945
1210.654730	163.389330	49.047949
1207.290184	162.809473	49.052954
1203.740569	168.220860	49.057959
1200.658327	164.061536	49.062964
1196.323723	164.224683	49.067969
1192.829245	156.194287	49.072973
1189.396089	150.958361	49.077978
1186.050121	166.291791	49.082983
1182.991515	162.670293	49.087988
1179.249221	163.420736	49.092993
1175.826302	161.173284	49.097997
1172.211779	167.465545	49.103002
1168.520265	160.172684	49.108007
1165.453413	153.166790	49.113012
1161.572043	152.135098	49.118017
1158.287043	154.487601	49.123021
1154.524970	157.185927	49.128026
1151.080402	165.527633	49.133031
1147.881466	149.441472	49.138036
1144.017144	163.062783	49.143041
1140.868375	160.216631	49.148045
1137.065319	156.138950	49.153050
1133.601961	169.165675	49.158055
1129.905171	149.999501	49.163060
1126.076612	161.426336	49.168065
1122.874023	153.164887	49.173069
1119.646496	154.380679	49.178074
1116.173375	152.466125	49.183079
1112.856075	156.115089	49.188084
1109.085853	164.808418	49.193089
1106.247344	156.916020	49.198093
1102.138685	157.878723	49.203098
1098.551872	166.188886	49.208103
1095.057921	151.497424	49.213108
1091.097928	159.714012	49.218113
1087.987563	154.707399	49.223117
1084.761093	161.713137	49.228122
1080.936011	162.420476	49.233127
1077.906381	162.745606	49.238132
1074.136589	156.786927	49.243137
1070.308302	157.631537	49.248141
1067.300417	150.937184	49.253146
1063.752792	162.531056	49.258151
1060.405365	149.619348	49.263156
1056.613179	154.752782	49.268161
1052.863945	159.097776	49.273165
1049.538164	159.693592	49.278170
1045.865280	159.223326	49.283175
1042.739735	146.414892	49.288180
1038.737554	157.036887	49.293185
1035.661719	153.282065	49.298189
1031.849377	154.055597	49.303194
1028.714615	151.565606	49.308199
1025.341170	153.992065	49.313204
1021.126616	154.785939	49.318209
1017.962954	147.490277	49.323213
1014.669974	149.142130	49.328218
1011.204191	149.986213	49.333223
1008.054414	145.315464	49.338228
1004.116370	154.962724	49.343233
1000.656417	148.972864	49.348237
997.260793	153.417052	49.353242
993.263574	153.891326	49.358247
989.639753	147.885713	49.363252
986.199267	153.503225	49.368257
983.039490	149.465336	49.373261
979.542746	146.795109	49.378266
976.047916	142.696925	49.383271
972.626232	151.250482	49.388276
969.054715	144.759839	49.393281
965.472748	152.844418	49.398285
962.062403	140.829293	49.403290
958.053916	146.480422	49.408295
955.051225	143.722516	49.413300
951.165336	153.198012	49.418305
947.941436	152.916187	49.423309
944.516608	154.760222	49.428314
940.529338	155.543846	49.433319
937.460202	146.069303	49.438324
933.718884	152.036226	49.443329
930.816241	154.930359	49.448333
927.396394	147.800171	49.453338
923.261941	162.615023	49.458343
920.088874	145.141789	49.463348
916.175786	155.128390	49.468353
913.052381	156.851143	49.473357
909.392509	146.896038	49.478362
905.911856	151.859424	49.483367
903.024686	143.811700	49.488372
899.053701	153.956444	49.493377
895.642369	143.453516	49.498381
891.865134	152.398288	49.503386
888.171980	159.876776	49.508391
884.670746	154.319201	49.513396
881.095977	156.654371	49.518401
877.679741	138.042789	49.523405
874.274092	145.582421	49.528410
870.934431	148.831882	49.533415
867.802662	136.325884	49.538420
863.919655	152.529933	49.543425
860.580883	141.395293	49.548429
856.885956	151.907935	49.553434
853.296882	147.373244	49.558439
849.941731	148.187991	49.563444
846.428364	146.263655	49.568449
842.830525	145.372282	49.573453
839.422946	139.026308	49.578458
835.871559	139.609072	49.583463
832.663806	140.942585	49.588468
828.662785	150.164270	49.593473
825.262889	144.800628	49.598477
821.972808	147.252385	49.603482
818.027830	150.305570	49.608487
814.894890	136.987074	49.613492
811.075736	154.086257	49.618497
807.971911	137.152465	49.623501
804.404221	138.988295	49.628506
800.337092	147.369810	49.633511
797.423331	140.965495	49.638516
793.743488	150.057897	49.643521
790.737832	148.162412	49.648525
786.993030	146.695613	49.653530
783.445442	144.892094	49.658535
779.940480	139.952586	49.663540
776.052432	149.059550	49.668545
772.972713	144.551876	49.673549
769.442765	136.360779	49.678554
765.540464	153.285870	49.683559
762.255498	134.427269	49.688564
758.680510	143.748513	49.693569
755.283054	145.087938	49.698573
751.968414	141.621015	49.703578
748.026837	149.606244	49.708583
744.800174	139.073212	49.713588
741.129233	140.360832	49.718593
737.928696	141.164701	49.723597
734.353565	145.192535	49.728602
730.525480	134.803433	49.733607
727.687111	140.654776	49.738612
723.647319	143.533563	49.743617
719.995452	133.124838	49.748621
716.854546	138.386074	49.753626
713.048578	144.343459	49.758631
710.288689	134.119598	49.763636
706.020421	137.891173	49.768641
702.659167	133.433784	49.773645
699.220725	138.492202	49.778650
695.532088	151.826007	49.783655
692.434393	140.268284	49.788660
688.805141	146.012800	49.793665
685.459641	138.249348	49.798669
681.865637	149.223579	49.803674
678.066487	151.298170	49.808679
675.105146	139.344725	49.813684
671.146350	138.325322	49.818689
667.653463	133.098578	49.823693
664.348900	142.229781	49.828698
660.781667	134.157970	49.833703
657.241941	130.893918	49.838708
653.540953	142.459408	49.843713
649.786646	140.421073	49.848717
646.340778	138.085950	49.853722
643.305439	140.552542	49.858727
639.871577	131.292220	49.863732
636.045114	141.156317	49.868737
632.708239	136.936842	49.873741
629.439607	143.006184	49.878746
625.818894	138.595144	49.883751
622.520192	135.070610	49.888756
618.352082	142.896107	49.893761
615.009659	135.885421	49.898765
611.566263	139.509663	49.903770
607.936793	140.907708	49.908775
604.799658	135.000516	49.913780
601.190740	140.444369	49.918785
597.474369	134.444521	49.923789
593.946304	146.256330	49.928794
590.286704	141.251516	49.933799
587.422814	136.123956	49.938804
583.715035	142.573460	49.943809
580.227995	134.508679	49.948813
576.700151	146.994865	49.953818
572.850590	143.751847	49.958823
569.574863	146.711992	49.963828
566.142008	148.072947	49.968833
562.747736	134.698923	49.973837
559.288359	133.469043	49.978842
555.530203	144.988477	49.983847
552.083669	123.554402	49.988852
548.685643	136.331293	49.993857
544.916041	138.599965	49.998861
541.488564	137.359300	50.003866
537.880673	139.062707	50.008871
534.666862	132.589608	50.013876
530.813982	143.161728	50.018881
527.443560	130.616736	50.023885
524.236486	131.223195	50.028890
520.358456	140.810556	50.033895
517.176745	126.273929	50.038900
513.498037	138.720929	50.043905
509.785335	133.852204	50.048909
506.407288	137.647128	50.053914
502.980656	134.674852	50.058919
500.110590	140.927615	50.063924
496.142634	137.847451	50.068929
492.440815	129.074545	50.073933
488.782606	135.942785	50.078938
485.513554	134.073792	50.083943
481.891460	139.342695	50.088948
478.127245	145.421853	50.093953
474.626407	131.823591	50.098957
471.660917	129.167311	50.103962
468.342574	134.028123	50.108967
464.888844	132.222204	50.113972
461.074298	140.269068	50.118977
457.414207	132.718826	50.123981
453.921957	138.477820	50.128986
450.107854	137.565074	50.133991
447.170010	132.280708	50.138996
443.586332	143.220283	50.144001
439.700652	140.841713	50.149005
436.628337	133.158476	50.154010
432.937486	131.492868	50.159015
429.607300	132.985210	50.164020
426.153515	144.451067	50.169025
422.533210	132.863137	50.174029
418.854010	133.388216	50.179034
415.372464	130.516909	50.184039
412.058741	139.946086	50.189044
408.288639	140.579318	50.194049
404.755788	132.926305	50.199053
401.441502	141.593373	50.204058
397.886972	133.033559	50.209063
394.874547	128.982001	50.214068
390.807096	140.600649	50.219073
387.433194	134.419758	50.224077
383.817534	127.759788	50.229082
380.532270	126.383547	50.234087
377.250302	135.488342	50.239092
373.269078	133.872712	50.244097
369.451613	136.425130	50.249101
366.601539	126.468025	50.254106
362.755151	136.062763	50.259111
359.702948	136.666013	50.264116
356.214211	137.206423	50.269121
352.478367	135.195604	50.274125
348.986076	134.454488	50.279130
345.207795	136.753414	50.284135
341.944635	136.638296	50.289140
338.254342	133.347806	50.294145
334.798994	127.841392	50.299149
331.532962	138.463153	50.304154
327.828206	131.319336	50.309159
324.202514	127.820874	50.314164
320.519131	134.817168	50.319169
317.190318	123.261464	50.324173
313.913695	124.330369	50.329178
310.037074	131.387498	50.334183
307.208293	121.887530	50.339188
303.509983	118.582606	50.344193
299.788518	127.904273	50.349197
296.640438	118.859479	50.354202
293.019999	123.451232	50.359207
289.760204	122.136438	50.364212
285.768205	120.697265	50.369217
282.069444	121.015815	50.374221
278.762585	115.113175	50.379226
274.840734	134.900199	50.384231
271.993888	120.990510	50.389236
268.528006	124.498867	50.394241
264.806264	130.900619	50.399245
260.998704	113.282018	50.404250
257.516247	133.273274	50.409255
254.468011	117.246497	50.414260
251.225853	118.333317	50.419265
247.355387	125.887666	50.424269
243.910449	119.544774	50.429274
240.661571	130.155148	50.434279
236.357842	125.428646	50.439284
233.190300	127.147164	50.444289
229.670162	139.456708	50.449293
226.585512	136.136360	50.454298
222.800022	138.545659	50.459303
219.331644	136.614440	50.464308
215.406714	131.427981	50.469313
211.855740	131.152028	50.474317
208.474095	126.340471	50.479322
205.156589	136.319863	50.484327
201.918732	127.660303	50.489332
198.715190	117.514473	50.494337
194.913394	124.437360	50.499341
191.492794	125.226754	50.504346
187.825643	125.698476	50.509351
184.146879	122.441399	50.514356
180.713501	124.513248	50.519361
176.910296	131.776738	50.524365
173.720443	131.202096	50.529370
169.984558	126.306145	50.534375
166.981948	130.239465	50.539380
163.474436	121.314714	50.544385
159.794505	117.899407	50.549389
156.243665	127.809245	50.554394
152.723104	129.549928	50.559399
149.302114	128.367008	50.564404
145.506343	130.383826	50.569409
142.473186	131.015206	50.574413
138.866595	125.951803	50.579418
135.090807	129.237770	50.584423
131.828415	129.851492	50.589428
127.947759	127.654508	50.594433
124.545043	125.770010	50.599437
121.123967	131.332523	50.604442
117.852577	122.789347	50.609447
114.084796	126.963471	50.614452
110.462145	129.227737	50.619457
106.881594	119.484916	50.624461
103.833205	124.881572	50.629466
100.018157	126.287674	50.634471
96.930877	126.339645	50.639476
93.453586	136.506196	50.644481
89.577669	132.449110	50.649485
86.046152	129.043356	50.654490
82.287652	124.057675	50.659495
78.882362	121.858428	50.664500
75.561936	136.068263	50.669505
71.714489	125.953047	50.674509
68.587905	125.886236	50.679514
65.334490	130.816910	50.684519
61.900212	127.316770	50.689524
58.402568	129.266120	50.694529
54.552954	132.137653	50.699533
51.217676	133.751091	50.704538
47.256157	131.336570	50.709543
44.155304	126.379954	50.714548
40.854074	126.439390	50.719553
37.322821	124.646523	50.724557
33.988177	125.329751	50.729562
29.832343	129.040744	50.734567
26.620564	132.761367	50.739572
22.792780	136.100188	50.744577
19.555181	137.577636	50.749581
16.207687	127.723647	50.754586
12.374871	125.935250	50.759591
8.905156	113.165916	50.764596
5.568729	128.746948	50.769601
1.911300	119.264723	50.774605