Thu Jun 16 10:52:02 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.525875	103.037528	0.000000
0.497917	101.583908	0.005005
0.584770	94.725786	0.010010
0.931059	103.527764	0.015014
0.625844	96.623842	0.020019
0.579696	99.701550	0.025024
-0.297609	85.022439	0.030029
0.072778	84.336913	0.035034
-0.489374	77.178216	0.040038
-0.718572	62.722710	0.045043
-0.747232	54.657132	0.050048
-1.093799	54.602102	0.055053
-1.354941	46.809448	0.060058
-1.420492	40.747811	0.065062
-2.112233	31.652866	0.070067
-2.120047	24.464738	0.075072
-2.558406	16.372277	0.080077
-2.869510	14.401749	0.085082
-3.049571	7.536279	0.090086
-3.355019	0.356604	0.095091
-3.514102	2.324755	0.100096
-4.059570	1.729024	0.105101
-4.306003	0.762266	0.110106
-4.603370	2.449416	0.115110
-4.752265	2.415684	0.120115
-4.876666	-2.747638	0.125120
-5.215696	5.139075	0.130125
-5.409995	4.658547	0.135130
-5.830072	7.578330	0.140134
-6.371179	-1.852937	0.145139
-6.044650	-4.708888	0.150144
-6.421334	5.382737	0.155149
-7.227619	-5.868663	0.160154
-7.758082	2.961044	0.165158
-7.937271	-1.219316	0.170163
-7.732675	-1.149279	0.175168
-7.832977	-4.285604	0.180173
-8.012456	3.327811	0.185178
-7.642309	-6.295479	0.190182
-8.720035	2.121832	0.195187
-9.189946	-2.753148	0.200192
-9.649892	1.102045	0.205197
-9.663774	-0.088514	0.210202
-9.941458	-8.540863	0.215206
-9.823982	3.915307	0.220211
-9.738580	-15.303509	0.225216
-9.877111	-0.171680	0.230221
-10.034373	-2.071835	0.235226
-10.808142	-9.796318	0.240230
-11.690601	4.853119	0.245235
-11.443259	-11.080073	0.250240
-11.393351	-11.859627	0.255245
-11.381151	-3.159261	0.260250
-12.288552	-2.203242	0.265254
-12.818381	-5.504068	0.270259
-12.711226	-7.154426	0.275264
-12.872932	-2.478496	0.280269
-13.267897	-9.756330	0.285274
-13.028475	-8.575489	0.290278
-13.398287	-1.356411	0.295283
-14.040401	-10.415727	0.300288
-14.255078	-0.310925	0.305293
-14.441961	-8.653779	0.310298
-14.677811	-7.084525	0.315302
-14.644936	-5.083973	0.320307
-14.934073	-4.805770	0.325312
-15.580558	2.361760	0.330317
-15.807641	-9.189764	0.335322
-15.749786	-4.263827	0.340326
-15.843005	-12.047995	0.345331
-15.861661	-5.845763	0.350336
-17.324979	-5.225338	0.355341
-17.299782	-11.739477	0.360346
-17.563396	-3.434808	0.365350
-17.677904	-6.144278	0.370355
-17.421957	-7.304846	0.375360
-17.701667	-12.827936	0.380365
-17.980434	-3.629133	0.385370
-17.821390	-12.428699	0.390374
-18.641850	-2.441022	0.395379
-19.041450	-5.394208	0.400384
-19.428371	4.582400	0.405389
-18.994587	-3.479759	0.410394
-19.157235	-11.758348	0.415398
-20.311274	-4.168856	0.420403
-20.664573	-17.787022	0.425408
-21.151387	-6.114338	0.430413
-20.950414	0.060577	0.435418
-20.627495	-19.754184	0.440422
-21.187380	-13.131431	0.445427
-20.689504	-13.418154	0.450432
-21.318506	-11.282275	0.455437
-22.364956	-5.189477	0.460442
-22.624797	-6.747123	0.465446
-22.934485	7.261317	0.470451
-22.869222	-5.756469	0.475456
-22.705111	-6.250452	0.480461
-22.892417	-4.663965	0.485466
-22.723023	-9.805791	0.490470
-23.578969	-4.375858	0.495475
-23.558329	-6.705353	0.500480
-24.286478	-8.626488	0.505485
-24.237565	-5.505615	0.510490
-24.344361	-10.778980	0.515494
-25.576232	-0.171049	0.520499
-25.418028	-4.830092	0.525504
-25.545668	3.891906	0.530509
-25.913179	0.471127	0.535514
-25.811507	2.797606	0.540518
-25.906512	1.726407	0.545523
-25.896443	2.462834	0.550528
-26.593617	4.469894	0.555533
-27.152574	5.238799	0.560538
-26.858421	-5.064381	0.565542
-27.448358	4.591612	0.570547
-27.446349	-8.523447	0.575552
-28.303049	-7.030547	0.580557
-28.828569	-6.710023	0.585562
-28.367117	-13.081292	0.590566
-28.808124	2.929411	0.595571
-28.762114	-7.941747	0.600576
-28.991449	-6.458608	0.605581
-28.825110	-13.057138	0.610586
-29.359688	-6.843734	0.615590
-30.370566	-4.369994	0.620595
-30.673533	-8.678665	0.625600
-30.916671	3.168819	0.630605
-30.968435	-4.575933	0.635610
-30.889728	-3.911324	0.640614
-31.230709	0.932447	0.645619
-30.735517	-13.398528	0.650624
-31.171544	-1.727724	0.655629
-31.706280	-4.537232	0.660634
-31.626639	-12.802982	0.665638
-32.534612	-6.660263	0.670643
-33.269652	-14.709789	0.675648
-33.373877	-4.203672	0.680653
-33.631105	-4.257481	0.685658
-33.449257	-5.260882	0.690662
-33.975905	-7.364481	0.695667
-33.546383	-6.308087	0.700672
-33.746282	-8.006157	0.705677
-33.892932	-1.168753	0.710682
-34.474771	-5.664159	0.715686
-35.211445	-1.791842	0.720691
-35.038217	-4.926904	0.725696
-35.232059	-0.292030	0.730701
-35.637994	-7.176887	0.735706
-36.195708	-8.884881	0.740710
-36.682057	-6.163588	0.745715
-36.691832	-11.175572	0.750720
-37.024164	-14.300973	0.755725
-37.150287	-2.429128	0.760730
-37.033194	-5.890038	0.765734
-37.273163	-4.106814	0.770739
-37.098523	3.726181	0.775744
-37.950942	-0.873574	0.780749
-38.345483	-4.707288	0.785754
-38.050103	-15.460522	0.790758
-38.580570	-3.440861	0.795763
-38.795112	-12.042446	0.800768
-39.446148	-5.996447	0.805773
-39.900513	2.157141	0.810778
-40.067980	-5.181176	0.815782
-40.526754	5.657798	0.820787
-40.402437	1.799500	0.825792
-40.464657	-4.487596	0.830797
-40.322979	5.800215	0.835802
-40.226230	-2.972881	0.840806
-40.884640	-1.253488	0.845811
-40.961796	-10.649938	0.850816
-41.242485	-4.077465	0.855821
-42.274595	-13.612548	0.860826
-42.727105	-1.382418	0.865830
-43.434196	1.527184	0.870835
-42.376119	1.768705	0.875840
-42.887682	-5.082517	0.880845
-43.424498	10.024674	0.885850
-43.537448	-3.811882	0.890854
-43.767243	-3.521189	0.895859
-43.582464	-6.263841	0.900864
-43.840409	-2.011409	0.905869
-44.586503	4.205485	0.910874
-44.546029	-1.959284	0.915878
-44.894461	2.225727	0.920883
-45.079951	-0.019981	0.925888
-45.408684	2.616961	0.930893
-46.440539	-0.390073	0.935898
-46.253615	-11.662949	0.940902
-46.902062	-1.662165	0.945907
-45.708350	-5.841523	0.950912
-46.422822	1.235927	0.955917
-46.553591	-1.264966	0.960922
-46.895272	-9.380487	0.965926
-47.946061	0.167184	0.970931
-48.455842	-1.844494	0.975936
-48.170634	-5.043442	0.980941
-48.317063	-6.836077	0.985946
-48.265514	-9.638593	0.990950
-48.527405	-2.753930	0.995955
-48.439215	-2.560775	1.000960
-49.200181	-3.676503	1.005965
-49.877551	2.203675	1.010970
-49.739729	-10.456145	1.015974
-50.275465	-3.029604	1.020979
-50.060498	-2.122630	1.025984
-50.155515	1.001115	1.030989
-50.552009	2.727735	1.035994
-50.903714	-6.173879	1.040998
-51.325553	6.460008	1.046003
-51.303970	-8.173107	1.051008
-51.710404	-2.893127	1.056013
-52.141248	-7.946212	1.061018
-52.155000	-9.327784	1.066022
-52.749036	-1.161573	1.071027
-52.948822	-10.350215	1.076032
-53.152765	-12.281621	1.081037
-53.396245	-7.381159	1.086042
-53.082529	-4.868643	1.091046
-53.578384	8.972367	1.096051
-53.322200	-5.577783	1.101056
-54.274098	-5.124541	1.106061
-54.313494	-11.454373	1.111066
-54.487572	-11.312680	1.116070
-55.310452	-4.903648	1.121075
-55.641614	-8.146935	1.126080
-56.003880	-6.784776	1.131085
-56.340224	-9.209271	1.136090
-56.044447	-10.538510	1.141094
-56.140621	-2.138197	1.146099
-56.020139	-8.035715	1.151104
-56.401770	-13.141917	1.156109
-56.199218	-3.668299	1.161114
-57.064777	-2.600016	1.166118
-57.608431	4.070771	1.171123
-57.702009	-2.652419	1.176128
-57.831697	-4.859107	1.181133
-58.844458	-2.951520	1.186138
-58.967873	-8.906988	1.191142
-59.301859	10.363593	1.196147
-58.671128	-11.545749	1.201152
-59.199812	-5.488302	1.206157
-59.214886	-0.071253	1.211162
-59.200464	-5.134097	1.216166
-59.813535	-2.619552	1.221171
-60.525045	1.979039	1.226176
-61.077748	-7.676510	1.231181
-61.387012	-9.872066	1.236186
-61.049628	-13.509665	1.241190
-61.388274	-1.558996	1.246195
-61.053240	-2.594818	1.251200
-61.278522	-8.625988	1.256205
-62.098770	-10.949496	1.261210
-62.222131	-9.949218	1.266214
-62.784504	-1.747299	1.271219
-62.633790	-14.773176	1.276224
-62.769415	-11.495828	1.281229
-62.874608	-18.838113	1.286234
-63.253660	-11.522905	1.291238
-64.208422	3.906199	1.296243
-64.209593	-14.937917	1.301248
-64.170200	-11.158344	1.306253
-64.345862	-4.765711	1.311258
-64.458410	-16.308528	1.316262
-65.067097	-2.504719	1.321267
-65.543549	-19.288631	1.326272
-66.072451	-10.631339	1.331277
-65.916899	1.300499	1.336282
-65.680341	-9.756241	1.341286
-66.041197	-8.581460	1.346291
-66.179526	-13.351410	1.351296
-66.926045	-13.534683	1.356301
-67.366123	-1.020218	1.361306
-67.579379	-7.037689	1.366310
-67.689055	-5.025319	1.371315
-67.515859	-8.640422	1.376320
-67.851286	-13.697533	1.381325
-68.492841	-11.777403	1.386330
-68.871943	-15.236312	1.391334
-69.172979	-10.375272	1.396339
-69.204274	-13.308524	1.401344
-69.172250	-12.112943	1.406349
-69.337638	-7.210590	1.411354
-69.387174	-9.679820	1.416358
-69.618588	-0.648861	1.421363
-70.012840	-1.290293	1.426368
-70.284915	-3.222080	1.431373
-70.453410	-7.677866	1.436378
-70.617194	-13.195939	1.441382
-71.878923	-3.195610	1.446387
-72.400463	-4.704182	1.451392
-72.129532	-17.341696	1.456397
-72.134902	-3.607213	1.461402
-72.254711	-14.372033	1.466406
-72.700942	-12.973997	1.471411
-72.961417	-5.940703	1.476416
-72.757179	-13.437518	1.481421
-72.769101	-5.761930	1.486426
-73.347171	-11.127482	1.491430
-73.751400	-5.591565	1.496435
-74.015790	-3.810914	1.501440
-74.124942	-8.021586	1.506445
-74.630875	10.311297	1.511450
-75.097357	-5.871797	1.516454
-75.655676	7.761017	1.521459
-75.904677	-8.977329	1.526464
-75.213132	-5.794955	1.531469
-75.329640	2.740126	1.536474
-75.686579	-3.586850	1.541478
-75.758871	6.367552	1.546483
-76.585827	-1.989378	1.551488
-76.845358	2.984079	1.556493
-77.183973	3.744886	1.561498
-77.228273	2.615883	1.566502
-77.316974	-2.206665	1.571507
-78.072590	2.516317	1.576512
-78.204752	1.523377	1.581517
-78.438506	-0.905347	1.586522
-78.962491	-11.465650	1.591526
-79.220473	-0.202313	1.596531
-79.080933	-3.351241	1.601536
-79.014303	3.270773	1.606541
-79.082773	-2.154044	1.611546
-79.244848	-12.167441	1.616550
-80.334893	2.177623	1.621555
-80.640624	9.067957	1.626560
-80.815891	-1.093714	1.631565
-80.971036	10.042439	1.636570
-80.615344	2.265074	1.641574
-80.971754	-2.288794	1.646579
-81.425549	-1.224237	1.651584
-82.052407	-1.673623	1.656589
-82.518786	8.871339	1.661594
-82.204004	-7.255995	1.666598
-82.451956	-1.271974	1.671603
-82.545386	-1.484062	1.676608
-83.043385	0.391333	1.681613
-83.426787	12.767599	1.686618
-83.367119	0.205435	1.691622
-83.727617	8.887685	1.696627
-83.775148	0.509471	1.701632
-84.207972	-4.934642	1.706637
-85.108636	9.902191	1.711642
-84.972938	-7.251927	1.716646
-85.237413	7.789531	1.721651
-85.241257	2.907281	1.726656
-84.949232	-3.041081	1.731661
-85.672500	1.950319	1.736666
-86.343720	4.167468	1.741670
-86.746877	8.765907	1.746675
-86.675511	0.855096	1.751680
-86.689980	-5.829964	1.756685
-86.923596	-0.138648	1.761690
-86.593394	-2.240609	1.766694
-87.719892	-0.681013	1.771699
-88.208884	-7.635203	1.776704
-87.982286	0.508045	1.781709
-88.707272	-4.024071	1.786714
-88.333651	1.604769	1.791718
-88.771905	4.087071	1.796723
-88.866760	1.243738	1.801728
-89.637493	-3.015933	1.806733
-90.143327	2.129636	1.811738
-90.377179	-0.125934	1.816742
-90.484016	-0.476090	1.821747
-90.319756	5.577724	1.826752
-90.149166	-4.671587	1.831757
-90.413411	1.722764	1.836762
-90.425808	-1.068296	1.841766
-91.303597	-5.817845	1.846771
-91.812630	-5.086683	1.851776
-91.743998	-7.899914	1.856781
-92.119589	-6.689746	1.861786
-91.961622	-4.848478	1.866790
-92.613873	9.901227	1.871795
-93.517494	-1.082304	1.876800
-93.132099	-4.998151	1.881805
-93.701851	0.474166	1.886810
-93.481662	-0.541690	1.891814
-93.933975	7.598144	1.896819
-93.919442	-4.988322	1.901824
-93.709633	0.772854	1.906829
-94.476137	0.047827	1.911834
-94.982031	-2.365218	1.916838
-95.418647	2.454701	1.921843
-95.959581	-1.202294	1.926848
-95.639449	-1.818745	1.931853
-95.475903	12.022001	1.936858
-95.455214	0.976861	1.941862
-96.367153	0.381331	1.946867
-96.571252	3.563355	1.951872
-96.579887	-1.729388	1.956877
-97.124264	5.269542	1.961882
-97.347622	-5.840620	1.966886
-98.041594	-0.404795	1.971891
-98.308549	0.842863	1.976896
-98.045024	-5.749730	1.981901
-98.607344	1.272289	1.986906
-98.598790	-6.089391	1.991910
-99.022412	4.948081	1.996915
-98.844174	-4.833632	2.006912
-98.764369	-4.774782	2.016909
-98.689788	-2.881669	2.026906
-97.529255	-3.530744	2.036902
-97.315386	0.158377	2.046899
-97.043571	-7.136056	2.056896
-95.985810	-1.520183	2.066893
-95.628244	-4.952774	2.076890
-95.732534	-1.531906	2.086886
-94.822036	-0.981070	2.096883
-94.256711	-7.454800	2.106880
-93.799945	-7.555105	2.116877
-93.001765	-1.004004	2.126874
-92.727258	0.756301	2.136870
-92.618856	-1.861122	2.146867
-91.644633	-0.858578	2.156864
-90.988341	-6.237701	2.166861
-90.968478	-1.130094	2.176858
-90.562695	-8.147662	2.186854
-89.647116	-1.171899	2.196851
-89.430144	-8.250868	2.206848
-88.959058	-6.023129	2.216845
-88.276770	-1.482845	2.226842
-87.824487	-8.529632	2.236838
-86.876073	-8.070902	2.246835
-86.368052	-1.939418	2.256832
-86.344351	-11.609440	2.266829
-86.288189	-4.045948	2.276826
-85.403899	-2.920178	2.286822
-84.869915	-8.432936	2.296819
-83.901171	-6.744053	2.306816
-83.417990	-3.133718	2.316813
-83.480210	-0.730516	2.326810
-83.232301	-5.379087	2.336806
-82.138454	-3.896043	2.346803
-81.963571	-3.845497	2.356800
-81.024481	-9.215102	2.366797
-80.395663	-6.195041	2.376794
-80.335875	-3.962150	2.386790
-80.137054	1.112919	2.396787
-78.940305	-6.843785	2.406784
-78.770007	-2.723500	2.416781
-78.835505	-1.916976	2.426778
-77.434642	-1.430881	2.436774
-77.119206	-4.030561	2.446771
-76.914001	-1.581915	2.456768
-75.851979	-2.392657	2.466765
-75.615562	0.943800	2.476762
-75.681516	-3.321987	2.486758
-75.006954	-1.400506	2.496755
-74.117693	-4.997375	2.506752
-74.068670	-1.496299	2.516749
-72.648145	-2.093855	2.526746
-72.395325	-9.359121	2.536742
-72.344007	-2.931484	2.546739
-72.118183	-4.345518	2.556736
-71.244570	-9.658072	2.566733
-70.811866	-4.418319	2.576730
-70.198535	-5.405214	2.586726
-69.384414	-9.875074	2.596723
-69.249131	2.658782	2.606720
-69.199360	2.948604	2.616717
-68.114781	-5.238142	2.626714
-67.966369	-2.990707	2.636710
-67.044501	-1.677339	2.646707
-66.452762	-8.342671	2.656704
-66.160393	-6.692938	2.666701
-66.245116	-9.258291	2.676698
-65.408183	-7.767900	2.686694
-64.870685	-5.227434	2.696691
-63.426611	-7.617138	2.706688
-63.803756	-6.483168	2.716685
-63.098643	-2.602352	2.726682
-62.923770	-5.388165	2.736678
-62.124482	-8.459372	2.746675
-61.530425	-11.728546	2.756672
-61.405236	2.665321	2.766669
-60.918366	3.022333	2.776666
-59.885616	3.336100	2.786662
-59.784578	2.942685	2.796659
-59.318005	-3.714903	2.806656
-58.506319	-0.415830	2.816653
-58.310957	-0.304511	2.826650
-58.032138	-4.674644	2.836646
-57.293952	-3.328548	2.846643
-56.763531	-0.271230	2.856640
-55.862263	-5.590231	2.866637
-55.331560	-7.435990	2.876634
-55.209988	-5.482977	2.886630
-55.188481	-0.779253	2.896627
-54.151759	2.532366	2.906624
-53.712526	-3.335503	2.916621
-53.379965	-6.526148	2.926618
-52.195251	1.791816	2.936614
-52.263658	-8.057437	2.946611
-52.006296	0.890249	2.956608
-51.097065	-5.732430	2.966605
-50.543706	-3.144402	2.976602
-50.394316	-4.919537	2.986598
-49.485112	-3.002999	2.996595
-49.035395	-4.247634	3.006592
-48.682711	-11.821940	3.016589
-48.354672	-2.543862	3.026586
-47.418822	1.594620	3.036582
-47.087541	-5.079972	3.046579
-46.809598	-0.572674	3.056576
-45.948315	-4.456761	3.066573
-45.631530	-6.612846	3.076570
-45.552927	-6.777582	3.086566
-44.290413	-5.642253	3.096563
-43.905088	-4.871315	3.106560
-43.814461	-2.762103	3.116557
-43.746203	0.422417	3.126554
-42.485728	3.066204	3.136550
-42.351524	-1.141640	3.146547
-41.112062	2.140872	3.156544
-40.725453	0.818357	3.166541
-40.781962	0.147429	3.176538
-40.657551	-3.306736	3.186534
-39.460455	-3.690248	3.196531
-39.015060	3.734644	3.206528
-38.997504	0.979570	3.216525
-38.323995	-4.569138	3.226522
-37.696010	0.430663	3.236518
-37.008687	-0.587126	3.246515
-36.235764	2.533936	3.256512
-35.749289	-5.206950	3.266509
-35.717822	4.419252	3.276506
-35.764669	2.073545	3.286502
-34.576600	-3.470507	3.296499
-34.150298	-5.519834	3.306496
-33.798520	4.813296	3.316493
-33.029950	4.946100	3.326490
-33.102888	-1.413211	3.336486
-32.099623	1.564436	3.346483
-31.340590	5.592222	3.356480
-31.295390	3.538064	3.366477
-30.750303	-2.856509	3.376474
-30.055965	1.867252	3.386470
-29.788907	-5.906221	3.396467
-29.026744	2.520401	3.406464
-28.590178	3.670732	3.416461
-28.242402	-1.207264	3.426458
-27.187638	-2.092317	3.436454
-26.754794	-0.417196	3.446451
-26.492527	-4.606345	3.456448
-26.463554	0.476103	3.466445
-25.786433	-6.149010	3.476442
-24.938323	2.239504	3.486438
-24.790950	-2.208378	3.496435
-23.897506	-9.348222	3.506432
-23.120913	-1.932725	3.516429
-22.962800	-1.838758	3.526426
-22.917932	-2.426623	3.536422
-22.540448	-1.868937	3.546419
-21.343998	2.279430	3.556416
-21.351488	-5.751679	3.566413
-20.527432	-1.228985	3.576410
-19.854853	-3.979057	3.586406
-19.935541	-0.366406	3.596403
-18.841824	-5.598030	3.606400
-18.279686	-3.986800	3.616397
-18.363228	-2.455016	3.626394
-18.013354	3.447318	3.636390
-17.038764	0.213988	3.646387
-16.512140	4.569905	3.656384
-15.908190	1.919138	3.666381
-15.115587	8.346470	3.676378
-15.312660	2.896343	3.686374
-14.864844	0.983926	3.696371
-13.566539	1.387167	3.706368
-13.559892	6.679313	3.716365
-13.482636	-3.751286	3.726362
-12.310551	-3.258089	3.736358
-11.828587	-1.020681	3.746355
-11.421128	-2.934034	3.756352
-11.410062	-3.696487	3.766349
-10.860268	3.685326	3.776346
-10.017527	1.588615	3.786342
-9.803811	1.671466	3.796339
-8.431368	1.239769	3.806336
-8.413031	5.631976	3.816333
-8.206598	-1.499735	3.826330
-8.064324	2.118546	3.836326
-7.138095	3.555765	3.846323
-6.896690	8.124226	3.856320
-5.985384	-0.000445	3.866317
-5.721689	6.822389	3.876314
-5.063955	11.280265	3.886310
-4.410675	16.567890	3.896307
-3.959429	20.229253	3.906304
-4.205088	22.084862	3.916301
-3.414441	34.921671	3.926298
-2.825300	47.572896	3.936294
-2.313116	58.342491	3.946291
-2.118343	61.681651	3.956288
-1.308348	78.362790	3.966285
-0.882418	92.213249	3.976282
-0.489989	109.428782	3.986278
0.000000	115.443775	3.991283
-0.455597	117.154719	3.996288
0.359621	133.148066	4.001293
0.751623	139.207614	4.006298
0.838815	140.630664	4.011302
0.823222	141.391465	4.016307
0.741806	151.211135	4.021312
0.884287	149.618850	4.026317
0.723711	140.253354	4.031322
0.900039	154.382275	4.036326
0.861673	145.190632	4.041331
0.267174	130.115999	4.046336
0.705053	146.143699	4.051341
0.530887	143.934768	4.056346
0.542040	148.628546	4.061350
1.029587	146.971640	4.066355
0.778118	146.749657	4.071360
0.786275	151.822862	4.076365
0.776683	136.135403	4.081370
0.333601	142.547234	4.086374
0.830571	139.085863	4.091379
0.668924	138.378751	4.096384
0.919283	139.967311	4.101389
0.813370	149.324393	4.106394
0.418569	152.306322	4.111398
0.860696	147.665226	4.116403
0.654922	148.731814	4.121408
0.478492	158.429666	4.126413
0.861571	161.058607	4.131418
0.961853	174.791092	4.136422
1.116796	180.543950	4.141427
1.248644	165.479275	4.146432
1.002830	170.122000	4.151437
1.512820	169.003392	4.156442
1.141848	155.709504	4.161446
1.339716	153.834497	4.166451
1.001772	156.701865	4.171456
1.233268	152.809242	4.176461
1.095537	141.611409	4.181466
1.067644	152.531998	4.186470
1.234247	147.815287	4.191475
0.845516	143.357767	4.196480
0.694758	147.580688	4.201485
1.090314	149.855862	4.206490
0.908888	150.811189	4.211494
1.315934	166.702142	4.216499
1.156000	162.119299	4.221504
1.388835	169.471394	4.226509
1.161275	153.172764	4.231514
1.378778	150.971814	4.236518
1.205981	153.885486	4.241523
0.832550	154.870964	4.246528
1.102760	169.719952	4.251533
1.628755	170.897746	4.256538
1.509104	171.165305	4.261542
1.467077	161.603415	4.266547
1.058680	157.198961	4.271552
1.092351	160.715526	4.276557
1.027514	161.726859	4.281562
0.952018	174.410790	4.286566
1.507279	176.503405	4.291571
1.434162	174.548873	4.296576
1.360135	175.732004	4.301581
1.574368	174.648263	4.306586
1.385905	176.509022	4.311590
1.642310	180.452065	4.316595
1.312056	173.268022	4.321600
1.306145	168.473267	4.326605
1.908287	175.494416	4.331610
1.643263	172.461438	4.336614
1.716815	160.169618	4.341619
1.437644	157.142730	4.346624
1.108342	150.113921	4.351629
1.252791	166.969703	4.356634
1.301548	172.255711	4.361638
1.186670	170.409104	4.366643
1.935781	160.881720	4.371648
1.897051	177.987192	4.376653
1.525556	176.997583	4.381658
1.695870	172.734555	4.386662
1.641975	170.921179	4.391667
1.143644	176.125940	4.396672
1.349449	167.502534	4.401677
1.648359	167.011722	4.406682
1.352261	185.953868	4.411686
1.478331	170.209326	4.416691
1.656889	184.958642	4.421696
1.295912	172.350119	4.426701
1.721548	175.268783	4.431706
1.804721	176.703451	4.436710
1.943313	178.926879	4.441715
1.701519	188.031095	4.446720
1.597630	179.289076	4.451725
1.804475	174.368102	4.456730
1.729388	176.357022	4.461734
1.517307	178.022402	4.466739
1.587254	193.740113	4.471744
1.558642	189.918780	4.476749
2.119484	201.627636	4.481754
1.719965	207.436617	4.486758
2.146362	198.489456	4.491763
2.188670	200.912988	4.496768
1.639691	190.903404	4.501773
1.806125	186.602440	4.506778
1.864758	189.078913	4.511782
2.284103	191.296297	4.516787
1.975512	179.911209	4.521792
1.840866	173.314590	4.526797
1.922780	176.817266	4.531802
1.667232	183.252777	4.536806
2.162880	185.797810	4.541811
2.083314	201.130229	4.546816
1.882974	193.481155	4.551821
2.108463	196.453024	4.556826
2.084855	201.041576	4.561830
1.996004	187.903477	4.566835
1.813581	188.449159	4.571840
1.730588	197.300528	4.576845
2.204032	199.905959	4.581850
2.002640	208.242093	4.586854
2.374126	200.616706	4.591859
2.407447	201.946063	4.596864
2.168005	195.332617	4.601869
2.137107	193.375940	4.606874
2.100315	207.065403	4.611878
2.152501	200.760004	4.616883
2.250927	200.834171	4.621888
2.033950	202.399636	4.626893
2.289956	202.791376	4.631898
2.195098	202.113080	4.636902
2.136652	208.313293	4.641907
2.439042	205.591616	4.646912
2.279324	204.037034	4.651917
2.687510	192.778839	4.656922
2.158060	192.197223	4.661926
1.940185	184.250649	4.666931
2.005534	195.421734	4.671936
2.099498	204.495532	4.676941
2.369796	201.462773	4.681946
2.101812	209.788899	4.686950
2.390845	202.677613	4.691955
2.063136	204.587826	4.696960
2.155712	208.727439	4.701965
2.411395	204.171201	4.706970
2.043258	206.886311	4.711974
2.407587	207.226707	4.716979
2.515840	211.282044	4.721984
2.144442	201.346792	4.726989
2.338612	197.560561	4.731994
2.565065	208.667346	4.736998
2.449859	203.158524	4.742003
2.592204	204.653067	4.747008
2.336598	202.220715	4.752013
2.683805	196.041380	4.757018
2.520755	208.170569	4.762022
2.376937	200.436878	4.767027
2.288062	206.845250	4.772032
2.660136	219.119235	4.777037
3.143363	215.859993	4.782042
2.357029	211.260392	4.787046
2.663848	204.386490	4.792051
2.224127	214.814328	4.797056
2.591906	223.041711	4.802061
3.274419	228.232971	4.807066
2.783517	222.655708	4.812070
2.525089	213.304364	4.817075
2.508779	211.632655	4.822080
2.382852	207.015372	4.827085
3.067253	214.781601	4.832090
2.514997	219.008443	4.837094
2.571821	226.144988	4.842099
2.915874	235.618759	4.847104
2.697887	226.881658	4.852109
3.007830	232.385369	4.857114
2.684604	226.703050	4.862118
2.815464	221.611415	4.867123
2.643898	231.452447	4.872128
2.794689	230.545123	4.877133
3.360932	222.721899	4.882138
2.676524	218.646673	4.887142
2.506780	210.056004	4.892147
3.076302	213.095722	4.897152
3.099506	232.472217	4.902157
3.048760	230.202823	4.907162
2.853314	216.416494	4.912166
2.595005	206.565447	4.917171
2.910713	221.245568	4.922176
2.948264	229.118601	4.927181
3.158492	231.706864	4.932186
2.718435	232.247769	4.937190
2.995558	235.188323	4.942195
2.712320	232.563026	4.947200
2.869301	234.429943	4.952205
3.201305	233.855723	4.957210
2.767502	235.476163	4.962214
3.273585	239.805235	4.967219
3.199330	244.691524	4.972224
3.284232	235.511717	4.977229
3.227403	236.062690	4.982234
2.934029	244.158034	4.987238
3.537176	229.035734	4.992243
3.270960	209.894375	4.997248
2.624948	212.409658	5.002253
3.448503	222.828118	5.007258
3.268751	238.834172	5.012262
3.231939	220.251950	5.017267
2.634624	225.104017	5.022272
2.825239	225.424780	5.027277
3.136954	235.121231	5.032282
3.135859	241.580223	5.037286
3.260211	245.232172	5.042291
3.305411	237.677065	5.047296
3.057465	244.107201	5.052301
3.171048	241.366208	5.057306
3.173316	246.087529	5.062310
3.152117	228.635474	5.067315
3.252244	236.526681	5.072320
3.231532	239.766547	5.077325
3.097052	237.392110	5.082330
3.127325	236.303545	5.087334
3.111576	230.902977	5.092339
3.431651	239.448325	5.097344
3.183581	238.549597	5.102349
3.615881	233.935652	5.107354
3.241384	242.766358	5.112358
3.428177	244.240832	5.117363
3.521828	249.151762	5.122368
3.482145	246.112902	5.127373
3.826540	238.440180	5.132378
3.557198	240.185074	5.137382
3.540905	232.730993	5.142387
3.551451	234.665123	5.147392
3.464292	232.396221	5.152397
3.319604	233.814290	5.157402
3.356603	240.446242	5.162406
3.287212	230.604606	5.167411
3.548196	243.125750	5.172416
3.867613	253.627939	5.177421
3.766918	244.522600	5.182426
3.295977	239.402159	5.187430
3.431830	244.817836	5.192435
3.789424	254.565911	5.197440
3.663584	259.090674	5.202445
3.607241	249.950577	5.207450
3.734150	257.083053	5.212454
3.859033	254.652729	5.217459
3.665478	225.847126	5.222464
3.631404	245.332646	5.227469
3.581150	241.038274	5.232474
3.541874	258.651704	5.237478
3.510233	250.144245	5.242483
3.422554	256.179720	5.247488
3.785305	264.191211	5.252493
3.687480	256.813928	5.257498
3.710820	268.307212	5.262502
3.831697	258.834063	5.267507
3.990168	262.123641	5.272512
3.838170	264.382179	5.277517
4.210265	259.517628	5.282522
3.786287	264.478291	5.287526
3.696044	249.771062	5.292531
3.589021	260.966142	5.297536
3.666834	259.810132	5.302541
3.710096	253.433970	5.307546
3.448863	264.002821	5.312550
3.690939	256.237591	5.317555
3.924401	256.566959	5.322560
3.570411	267.429448	5.327565
3.758542	275.992477	5.332570
3.807626	292.939135	5.337574
3.925819	291.049260	5.342579
4.245778	290.337136	5.347584
4.158975	292.644986	5.352589
4.501135	287.240795	5.357594
3.790009	288.937751	5.362598
4.025369	271.039552	5.367603
4.039737	272.780283	5.372608
4.190060	288.575275	5.377613
4.043317	271.199462	5.382618
3.872494	279.112777	5.387622
3.961200	283.041632	5.392627
4.238399	288.267140	5.397632
4.187538	289.529519	5.402637
4.134890	287.904256	5.407642
4.244828	294.844314	5.412646
4.090310	289.248334	5.417651
4.092442	291.137593	5.422656
4.108995	288.607174	5.427661
4.322943	287.641070	5.432666
4.140065	296.708483	5.437670
3.880584	284.151956	5.442675
4.148630	284.055141	5.447680
3.806033	285.809779	5.452685
4.437947	290.273848	5.457690
4.289199	290.805780	5.462694
4.160279	292.161069	5.467699
4.262946	302.603119	5.472704
4.156293	291.489126	5.477709
4.652841	295.719063	5.482714
4.465656	292.281141	5.487718
4.422170	296.762215	5.492723
4.367221	289.347150	5.497728
4.200433	287.148915	5.502733
4.389778	291.476480	5.507738
3.962838	289.089989	5.512742
4.411455	288.861718	5.517747
4.510104	286.359859	5.522752
4.313410	289.814487	5.527757
4.315426	285.962911	5.532762
4.164656	296.756419	5.537766
4.249678	299.869711	5.542771
4.639040	304.824822	5.547776
4.529238	315.913657	5.552781
4.775653	308.613238	5.557786
4.511361	299.666903	5.562790
4.615663	287.961042	5.567795
4.442471	286.350274	5.572800
4.765365	288.708410	5.577805
4.779574	280.934850	5.582810
4.421131	291.984254	5.587814
4.492501	294.512900	5.592819
4.327637	298.994501	5.597824
4.308188	312.153483	5.602829
4.739563	315.021602	5.607834
4.902597	328.351305	5.612838
4.788016	326.369668	5.617843
4.964535	320.386896	5.622848
4.735117	310.573825	5.627853
4.512769	305.880597	5.632858
4.620471	324.046257	5.637862
5.025812	329.898968	5.642867
5.052931	310.880372	5.647872
4.917026	302.349468	5.652877
4.909191	297.911334	5.657882
4.452085	297.891439	5.662886
4.443458	291.294957	5.667891
4.622750	299.020593	5.672896
4.719045	322.154351	5.677901
4.939539	317.347489	5.682906
4.809001	334.426379	5.687910
4.647363	318.986821	5.692915
4.992552	330.264380	5.697920
4.675625	335.021310	5.702925
4.975953	324.073851	5.707930
4.910145	333.751067	5.712934
4.775499	330.988532	5.717939
4.809362	322.061576	5.722944
4.945917	328.972884	5.727949
5.143384	332.349853	5.732954
4.722750	322.165761	5.737958
4.521556	331.797867	5.742963
4.858327	330.881903	5.747968
4.624111	327.539746	5.752973
4.746296	321.840609	5.757978
4.592719	334.168800	5.762982
5.014372	335.296568	5.767987
5.116886	359.243362	5.772992
5.153896	360.900252	5.777997
5.415430	352.602765	5.783002
5.130485	354.638030	5.788006
5.076172	346.738332	5.793011
5.116834	334.385413	5.798016
4.782484	346.510266	5.803021
5.046356	349.061567	5.808026
5.196303	361.750917	5.813030
5.257638	361.573623	5.818035
5.306761	361.029474	5.823040
5.639557	360.060694	5.828045
5.376546	343.415321	5.833050
5.015455	344.242106	5.838054
5.057856	327.016498	5.843059
5.276093	348.337770	5.848064
5.302093	358.040771	5.853069
5.314826	355.382720	5.858074
5.282509	355.574782	5.863078
5.378572	356.352855	5.868083
5.466912	350.442554	5.873088
5.043585	333.143553	5.878093
5.404395	342.501660	5.883098
5.316923	355.737823	5.888102
5.520352	359.036566	5.893107
5.571423	360.498557	5.898112
5.384677	350.318019	5.903117
5.220631	327.492201	5.908122
5.519401	341.935207	5.913126
5.406182	340.930035	5.918131
5.491980	342.548080	5.923136
5.302015	341.881549	5.928141
5.336303	345.265066	5.933146
5.339531	363.084096	5.938150
5.496628	350.547167	5.943155
5.771188	358.175304	5.948160
5.644482	360.332600	5.953165
5.494438	364.586539	5.958170
5.757824	364.198276	5.963174
5.603759	356.952966	5.968179
5.436985	339.381101	5.973184
5.146426	348.642046	5.978189
5.358243	363.059289	5.983194
5.525329	350.419094	5.988198
5.276249	365.118794	5.993203
5.825082	361.457806	5.998208
5.509913	354.114224	6.003213
5.420939	354.593167	6.008218
5.390516	363.430518	6.013222
5.405241	369.107470	6.018227
5.682885	357.030871	6.023232
5.654566	360.120286	6.028237
5.367112	358.919562	6.033242
5.361666	366.214151	6.038246
5.295896	369.917082	6.043251
5.403790	365.722327	6.048256
5.427520	364.312624	6.053261
5.834868	376.562162	6.058266
5.642845	364.941419	6.063270
5.146097	373.969688	6.068275
5.738269	368.929924	6.073280
5.690001	382.895012	6.078285
5.794049	372.695112	6.083290
5.717890	362.392011	6.088294
5.674540	370.665810	6.093299
5.758577	362.479633	6.098304
5.542124	363.405442	6.103309
5.679886	358.894493	6.108314
5.932943	366.958892	6.113318
5.451744	366.020251	6.118323
5.943141	355.190560	6.123328
5.598834	366.087724	6.128333
5.632260	364.540570	6.133338
5.547276	362.652200	6.138342
5.711395	368.580108	6.143347
5.827889	355.513789	6.148352
5.671211	359.106152	6.153357
5.802318	355.882085	6.158362
5.716497	354.622587	6.163366
5.449937	363.503302	6.168371
5.802000	361.647677	6.173376
5.714684	366.811511	6.178381
5.677597	371.671770	6.183386
5.752047	360.101014	6.188390
5.464101	363.003565	6.193395
5.827824	350.678241	6.198400
5.464945	369.884701	6.203405
5.673485	353.446308	6.208410
5.694842	357.550870	6.213414
5.356562	359.317923	6.218419
5.634748	355.213909	6.223424
5.787803	366.232408	6.228429
5.848411	354.044484	6.233434
5.751318	360.907403	6.238438
5.796642	355.405640	6.243443
5.734283	356.178520	6.248448
5.425922	361.227643	6.253453
5.336752	355.768034	6.258458
5.519702	367.866314	6.263462
5.199441	358.323743	6.268467
5.318199	363.575953	6.273472
5.338403	364.149520	6.278477
5.234245	369.724672	6.283482
5.231612	361.082921	6.288486
5.234076	368.226444	6.293491
5.561164	374.626424	6.298496
5.810054	377.969354	6.303501
5.642925	375.806383	6.308506
5.434751	366.429179	6.313510
5.413401	379.749638	6.318515
5.657153	385.440444	6.323520
5.732299	385.448413	6.328525
5.526328	385.045075	6.333530
5.936431	388.803739	6.338534
5.568752	390.655073	6.343539
5.582090	374.286899	6.348544
5.676912	368.469934	6.353549
5.583711	368.956383	6.358554
5.436952	369.833877	6.363558
5.436685	381.435130	6.368563
5.876327	380.576352	6.373568
5.455963	390.130569	6.378573
5.386842	383.079375	6.383578
5.844732	391.352531	6.388582
5.522597	381.611168	6.393587
6.094902	375.969431	6.398592
5.421056	378.903792	6.403597
5.509653	360.450732	6.408602
5.655527	365.877128	6.413606
5.388470	379.188765	6.418611
5.839059	372.298231	6.423616
5.527262	386.872566	6.428621
5.708291	365.900236	6.433626
5.712739	362.681511	6.438630
5.419464	375.258349	6.443635
5.604587	358.157400	6.448640
5.299488	371.058990	6.453645
5.692882	375.665597	6.458650
5.796139	379.936775	6.463654
5.565663	388.036599	6.468659
6.016079	375.492020	6.473664
5.428601	380.300877	6.478669
5.796869	364.126026	6.483674
5.710135	365.690110	6.488678
5.480051	359.123290	6.493683
5.590157	368.529650	6.498688
5.406496	371.586433	6.503693
5.641456	360.373909	6.508698
5.719263	367.543556	6.513702
5.295298	371.359646	6.518707
5.666922	365.772386	6.523712
5.600728	389.947971	6.528717
5.388791	386.590675	6.533722
6.004081	391.621735	6.538726
5.449950	384.764046	6.543731
5.748185	378.270423	6.548736
5.762088	378.477242	6.553741
5.510745	361.742018	6.558746
5.227875	369.110374	6.563750
5.298380	377.107573	6.568755
5.916349	379.838715	6.573760
5.495066	387.267541	6.578765
5.652611	385.724538	6.583770
5.812408	391.325236	6.588774
5.863390	396.600497	6.593779
5.983475	372.016667	6.598784
5.488668	385.458683	6.603789
5.170943	372.712621	6.608794
5.722999	373.601897	6.613798
5.446018	377.483772	6.618803
5.847375	380.579235	6.623808
5.373445	383.499798	6.628813
5.448532	376.879283	6.633818
5.897037	384.500589	6.638822
5.574840	392.602648	6.643827
6.021012	377.853314	6.648832
5.637052	382.464474	6.653837
5.596873	367.702391	6.658842
5.617020	373.800696	6.663846
5.124641	382.765107	6.668851
5.759266	374.811231	6.673856
5.663912	384.477576	6.678861
5.530286	374.251248	6.683866
5.735805	370.705693	6.688870
5.328159	376.662485	6.693875
5.830700	372.775035	6.698880
5.580790	386.654076	6.703885
5.861744	377.718317	6.708890
5.734120	365.274106	6.713894
5.306877	378.215617	6.718899
5.182200	371.861438	6.723904
5.602686	377.957712	6.728909
5.731064	388.144196	6.733914
5.648545	393.874519	6.738918
5.523320	409.460738	6.743923
5.966873	404.594789	6.748928
5.679886	380.778280	6.753933
5.498392	372.234548	6.758938
5.631793	372.412148	6.763942
5.575605	375.190275	6.768947
5.491948	374.648732	6.773952
5.822245	387.702331	6.778957
5.768409	382.917698	6.783962
5.976441	373.964494	6.788966
5.635307	377.816127	6.793971
5.952229	371.953480	6.798976
5.799215	363.277385	6.803981
5.771866	369.535566	6.808986
5.711335	374.414893	6.813990
5.511237	373.110251	6.818995
5.687041	378.285756	6.824000
5.380925	375.296918	6.829005
5.531138	375.746891	6.834010
5.607769	371.905852	6.839014
5.478070	365.484038	6.844019
5.859259	370.192796	6.849024
5.691496	360.354310	6.854029
5.610572	368.787036	6.859034
5.729416	379.665780	6.864038
5.607559	370.158980	6.869043
5.910478	368.720108	6.874048
5.759647	371.449354	6.879053
6.068832	363.397138	6.884058
5.876400	370.466913	6.889062
5.633095	361.543119	6.894067
5.765042	349.211803	6.899072
5.179135	346.363424	6.904077
5.157395	369.070342	6.909082
5.734883	360.210882	6.914086
5.438479	375.130424	6.919091
5.707380	369.422710	6.924096
5.914984	375.511347	6.929101
5.565215	373.735595	6.934106
5.691186	366.939848	6.939110
5.386010	377.878895	6.944115
5.773429	374.747329	6.949120
5.580582	377.328334	6.954125
5.670959	382.404109	6.959130
5.888128	369.841945	6.964134
5.751234	380.718952	6.969139
5.870181	354.181063	6.974144
5.550401	352.064040	6.979149
5.369092	360.512759	6.984154
5.704188	347.262831	6.989158
5.028031	354.183262	6.994163
5.438741	363.415834	6.999168
5.469519	370.677703	7.004173
5.773683	367.033963	7.009178
5.775461	369.139049	7.014182
5.391340	376.234290	7.019187
5.430873	367.032798	7.024192
5.765473	376.283283	7.029197
5.604027	368.868612	7.034202
5.540477	379.282541	7.039206
5.188728	380.668248	7.044211
5.397659	368.753051	7.049216
5.136230	378.016401	7.054221
5.152536	372.183405	7.059226
5.615253	369.465196	7.064230
5.269295	380.146587	7.069235
5.659182	375.194017	7.074240
5.502581	385.225250	7.079245
5.507656	389.531895	7.084250
5.705080	396.971540	7.089254
5.647366	405.578821	7.094259
5.912076	386.233187	7.099264
5.788960	379.272308	7.104269
5.792969	379.277235	7.109274
5.872567	367.901355	7.114278
5.644110	378.219807	7.119283
5.834867	365.057844	7.124288
5.650036	381.720355	7.129293
5.449183	376.922431	7.134298
5.668197	366.042345	7.139302
5.607540	374.631251	7.144307
5.707686	374.340503	7.149312
5.589769	375.493708	7.154317
5.924715	379.424021	7.159322
5.950544	368.277424	7.164326
5.854212	378.465619	7.169331
6.033507	371.634125	7.174336
6.135679	374.831415	7.179341
5.685741	356.911799	7.184346
5.755360	346.581955	7.189350
5.275041	338.075490	7.194355
5.755530	343.930881	7.199360
5.400453	346.840281	7.204365
5.372196	345.998648	7.209370
5.711095	357.690732	7.214374
5.521763	352.706820	7.219379
5.882379	359.321058	7.224384
5.611039	357.374103	7.229389
5.430082	341.941167	7.234394
5.386627	353.572523	7.239398
5.543637	365.473633	7.244403
6.187426	372.260490	7.249408
5.919230	355.314765	7.254413
5.705902	346.709221	7.259418
5.492629	341.379338	7.264422
5.600470	344.141403	7.269427
5.397307	349.399848	7.274432
5.639041	332.240837	7.279437
5.190399	340.025277	7.284442
5.681122	342.368512	7.289446
5.125271	358.589661	7.294451
5.583383	358.370476	7.299456
5.542040	372.078497	7.304461
5.461609	371.447828	7.309466
5.863420	372.257061	7.314470
5.649077	385.978590	7.319475
6.052082	371.544893	7.324480
5.550979	366.222413	7.329485
5.337596	362.497671	7.334490
5.810906	372.194339	7.339494
5.580467	380.560524	7.344499
5.541779	366.577873	7.349504
5.679267	382.949754	7.354509
5.538880	374.652280	7.359514
5.704612	363.264143	7.364518
5.368135	378.450761	7.369523
5.291774	367.976818	7.374528
5.760838	374.351066	7.379533
5.694913	367.734127	7.384538
5.432732	375.897784	7.389542
5.339540	384.208141	7.394547
5.394846	379.572201	7.399552
5.387006	374.662470	7.404557
5.397713	374.913029	7.409562
5.607783	383.502188	7.414566
5.550810	374.675649	7.419571
5.764812	378.744927	7.424576
5.988893	382.576950	7.429581
5.587265	384.214680	7.434586
5.656223	371.367425	7.439590
5.572333	382.855726	7.444595
5.913204	378.766405	7.449600
5.806760	374.212148	7.454605
5.892293	375.272145	7.459610
5.905640	370.403703	7.464614
5.423098	378.536693	7.469619
5.511082	371.885537	7.474624
5.269745	382.211645	7.479629
5.512374	372.172146	7.484634
5.562146	366.807071	7.489638
5.698590	380.763633	7.494643
5.357288	372.077017	7.499648
5.612036	377.739365	7.504653
5.766855	382.405033	7.509658
6.284583	362.384048	7.514662
5.544596	381.577468	7.519667
6.019162	369.860968	7.524672
5.432073	357.290744	7.529677
5.503394	344.061620	7.534682
5.789710	343.952216	7.539686
5.371388	352.333747	7.544691
5.593757	362.595839	7.549696
5.632633	358.228005	7.554701
5.837464	363.559813	7.559706
5.743796	337.409389	7.564710
5.515733	351.769385	7.569715
5.689161	350.789650	7.574720
5.572356	343.381623	7.579725
5.099764	344.437760	7.584730
5.704201	368.467463	7.589734
5.604038	371.506698	7.594739
5.751477	368.165982	7.599744
5.870086	371.724299	7.604749
5.395089	370.185200	7.609754
5.695434	355.376030	7.614758
5.621346	344.495167	7.619763
5.667326	344.874856	7.624768
5.220925	351.984029	7.629773
5.790736	359.712344	7.634778
5.926433	377.519958	7.639782
5.744056	354.322138	7.644787
5.692676	349.335161	7.649792
5.669832	347.009147	7.654797
5.594031	337.284620	7.659802
5.596535	345.166958	7.664806
5.267152	352.804430	7.669811
5.476347	343.528251	7.674816
5.368728	350.029260	7.679821
5.450587	376.486041	7.684826
5.850960	369.237300	7.689830
5.970873	377.376981	7.694835
5.873020	364.924003	7.699840
5.386952	350.253973	7.704845
5.216612	350.239864	7.709850
5.662509	357.012655	7.714854
5.763301	371.255183	7.719859
5.913020	374.054037	7.724864
5.791255	355.610687	7.729869
5.353157	353.977195	7.734874
5.605834	338.467570	7.739878
5.224145	346.357264	7.744883
5.381198	354.995026	7.749888
6.281855	365.827924	7.754893
5.588789	361.904441	7.759898
5.464495	345.374556	7.764902
5.216970	352.762418	7.769907
5.563497	369.688616	7.774912
5.641992	374.215556	7.779917
5.660411	385.650449	7.784922
6.258893	373.767949	7.789926
5.504093	369.348463	7.794931
5.452160	346.169153	7.799936
5.236128	354.456188	7.804941
5.521236	366.409529	7.809946
5.632760	370.949064	7.814950
5.480657	370.646629	7.819955
5.632230	377.512759	7.824960
5.887281	378.238513	7.829965
5.704803	363.349698	7.834970
5.941008	362.084140	7.839974
5.567591	350.564022	7.844979
5.528823	347.257536	7.849984
5.506915	345.590683	7.854989
5.110533	355.113095	7.859994
5.820631	362.337874	7.864998
5.797567	372.017817	7.870003
5.781075	358.788887	7.875008
5.751929	350.657824	7.880013
5.707718	354.318713	7.885018
5.622831	341.888571	7.890022
5.335847	343.336380	7.895027
5.332679	343.341112	7.900032
5.397497	355.958299	7.905037
5.074442	374.958307	7.910042
5.523734	374.986726	7.915046
5.682053	390.661819	7.920051
5.508646	379.781855	7.925056
5.609932	385.598806	7.930061
5.372004	385.162668	7.935066
5.667810	375.310212	7.940070
5.608175	388.588270	7.945075
5.603611	377.435048	7.950080
5.765433	377.567206	7.955085
6.003706	377.807288	7.960090
5.824190	373.783445	7.965094
5.757399	384.629631	7.970099
5.422975	377.836563	7.975104
5.531375	380.711502	7.980109
5.409642	385.409357	7.985114
5.841839	378.238224	7.990118
5.810782	384.835312	7.995136
5.926782	373.547249	8.000154
5.781008	379.889547	8.005171
5.247823	375.053774	8.010189
5.854157	367.505819	8.015206
5.417546	376.653365	8.020224
5.725821	374.078910	8.025242
5.674638	378.427946	8.030259
5.252873	386.457731	8.035277
5.814592	374.886408	8.040294
5.623500	388.003163	8.045312
5.465297	370.587121	8.050330
5.777814	375.145090	8.055347
5.475515	376.668814	8.060365
5.561045	377.413048	8.065382
5.466752	386.306237	8.070400
5.518311	379.661398	8.075418
5.622679	382.808996	8.080435
5.455173	382.679100	8.085453
5.780157	372.016106	8.090470
5.610068	378.511996	8.095488
5.923537	379.393328	8.100506
5.962804	378.931096	8.105523
5.462385	385.064442	8.110541
5.634668	381.334659	8.115558
5.733492	389.530919	8.120576
5.449014	373.145666	8.125594
5.559510	384.233768	8.130611
5.472301	384.467983	8.135629
5.693474	375.412257	8.140646
5.757217	381.412123	8.145664
5.777700	371.286748	8.150682
6.068200	369.326616	8.155699
5.519119	376.771463	8.160717
5.576526	374.983287	8.165734
5.744489	381.787310	8.170752
5.861288	396.246202	8.175770
5.928122	379.219742	8.180787
5.653420	380.401576	8.185805
6.006650	388.353573	8.190822
6.022913	379.040234	8.195840
5.688691	374.858836	8.200858
6.110477	380.227017	8.205875
5.995405	383.915496	8.210893
5.857999	379.174420	8.215910
5.515804	377.342462	8.220928
6.060889	376.938342	8.225946
5.822958	370.898709	8.230963
5.283052	376.724963	8.235981
5.988977	390.234115	8.240998
5.864476	391.939241	8.246016
5.965351	391.126053	8.251034
5.931244	377.737752	8.256051
5.493014	378.811403	8.261069
5.736337	385.961165	8.266086
5.877808	395.419994	8.271104
5.823236	395.652161	8.276122
6.286142	394.068961	8.281139
6.123437	403.891972	8.286157
5.923528	384.426352	8.291174
5.777744	381.213894	8.296192
5.942227	402.860627	8.301210
6.088434	386.959383	8.306227
5.630448	386.541144	8.311245
6.239718	398.153592	8.316262
6.009251	389.736745	8.321280
5.738622	383.471555	8.326298
6.119116	385.047074	8.331315
5.773463	397.386794	8.336333
5.925442	391.083547	8.341350
6.207395	401.913455	8.346368
5.819203	404.054103	8.351386
6.440713	391.379713	8.356403
6.023456	383.164665	8.361421
5.864805	391.789418	8.366438
5.829682	386.162232	8.371456
5.890959	393.345724	8.376474
6.258713	387.905055	8.381491
5.767597	390.628535	8.386509
5.796082	385.926170	8.391526
6.104528	399.364529	8.396544
6.092812	402.774176	8.401562
6.274937	401.839316	8.406579
6.364257	405.773098	8.411597
6.107972	382.719722	8.416614
6.092610	388.303227	8.421632
5.968980	386.296792	8.426650
5.856035	377.672085	8.431667
6.053986	379.395954	8.436685
5.959814	382.044487	8.441702
6.009877	387.555972	8.446720
6.157874	388.722568	8.451738
6.312529	397.346817	8.456755
6.289384	393.667630	8.461773
6.303212	384.055442	8.466790
6.293036	382.899857	8.471808
5.956986	383.559561	8.476826
6.021139	381.761019	8.481843
5.831941	383.392109	8.486861
5.884878	382.636637	8.491878
5.837424	380.857228	8.496896
5.953533	394.766546	8.501914
6.273646	399.619858	8.506931
5.899701	396.763342	8.511949
6.262242	403.688337	8.516966
6.015870	396.400549	8.521984
6.388060	389.662177	8.527002
6.405527	401.016399	8.532019
6.270703	402.570508	8.537037
6.177472	410.173946	8.542054
6.320029	400.440496	8.547072
5.878306	403.296140	8.552090
6.037243	408.462348	8.557107
6.139605	402.206757	8.562125
6.130193	402.764756	8.567143
6.429418	402.099558	8.572160
6.363274	402.160052	8.577178
6.358135	397.996986	8.582195
6.274225	404.718063	8.587213
6.500729	404.653341	8.592231
6.529992	402.758714	8.597248
6.108644	397.712170	8.602266
6.233027	403.392050	8.607283
6.226451	399.652851	8.612301
6.237419	398.042193	8.617319
6.525700	394.500181	8.622336
6.141240	411.084502	8.627354
6.289417	397.940904	8.632371
6.388369	403.391276	8.637389
6.123645	404.449441	8.642407
6.089441	406.361942	8.647424
6.100540	411.891093	8.652442
6.163844	405.476045	8.657459
5.970115	410.783390	8.662477
6.340560	410.676578	8.667495
6.070589	413.782227	8.672512
6.055544	413.144068	8.677530
6.142745	408.167285	8.682547
6.364499	413.224808	8.687565
6.092170	413.204832	8.692583
6.025484	414.244638	8.697600
6.045791	414.116670	8.702618
6.306722	428.884381	8.707635
6.315326	430.378380	8.712653
6.266450	433.943554	8.717671
6.460017	438.163498	8.722688
6.139087	438.564755	8.727706
6.497535	436.218957	8.732723
6.475461	431.396023	8.737741
6.182461	439.406327	8.742759
6.738886	441.602250	8.747776
6.436045	441.872395	8.752794
6.765406	441.646118	8.757811
6.651356	436.769106	8.762829
6.641440	429.156854	8.767847
6.842123	409.515280	8.772864
6.055748	416.795663	8.777882
6.204009	406.395462	8.782899
6.603569	422.631183	8.787917
6.435059	429.285068	8.792935
6.431506	428.143244	8.797952
6.599583	448.492868	8.802970
6.447735	430.700098	8.807987
6.287638	442.952213	8.813005
6.280668	438.213968	8.818023
6.827974	436.521659	8.823040
6.655013	444.176962	8.828058
6.923263	435.255124	8.833075
6.431590	425.739831	8.838093
6.178358	409.066266	8.843111
6.344659	424.929206	8.848128
6.433335	440.207281	8.853146
6.461674	436.363604	8.858163
6.607759	435.961655	8.863181
6.585429	435.674035	8.868199
6.430347	429.480263	8.873216
6.381369	438.143599	8.878234
6.205438	439.135530	8.883251
6.356450	435.094747	8.888269
6.411240	440.303368	8.893287
6.352015	432.592297	8.898304
6.424721	427.723000	8.903322
6.490180	434.153615	8.908339
6.729444	436.609386	8.913357
6.345339	445.157769	8.918375
6.482658	439.372960	8.923392
6.355756	453.808511	8.928410
6.621390	458.898848	8.933427
6.721626	461.766002	8.938445
6.622706	455.498583	8.943463
7.273109	456.473913	8.948480
6.860780	452.433918	8.953498
6.671662	436.238504	8.958515
6.769835	428.194795	8.963533
6.585806	433.160262	8.968551
6.700848	436.882463	8.973568
6.261496	440.451352	8.978586
6.426509	453.479596	8.983603
6.626835	461.176545	8.988621
6.800050	469.115723	8.993639
6.930901	462.444559	8.998656
6.838530	469.702975	9.003674
6.708687	464.028828	9.008691
6.714537	457.891307	9.013709
6.646511	468.459086	9.018727
6.894387	464.724663	9.023744
7.183501	476.829456	9.028762
6.945655	451.995835	9.033779
6.770219	448.887160	9.038797
6.476517	448.707857	9.043815
6.809236	433.983857	9.048832
6.563117	440.667694	9.053850
6.768443	451.157618	9.058867
7.144741	453.829673	9.063885
6.765952	446.825993	9.068903
7.023164	435.008257	9.073920
6.779146	434.680221	9.078938
7.000358	445.186015	9.083955
6.871052	437.263144	9.088973
6.500980	430.769735	9.093991
6.914077	435.429383	9.099008
6.484428	442.797843	9.104026
6.910929	451.712561	9.109043
7.083462	439.789155	9.114061
6.669054	442.408844	9.119079
6.875149	445.513370	9.124096
6.924971	444.691691	9.129114
7.029118	455.829998	9.134131
6.883326	437.314223	9.139149
7.092822	439.572595	9.144167
6.699796	436.594054	9.149184
7.017501	433.132881	9.154202
6.634363	443.565257	9.159219
7.140806	442.377037	9.164237
6.851589	450.554502	9.169255
6.950420	455.233420	9.174272
7.193500	442.496650	9.179290
6.667099	445.880459	9.184307
7.026684	448.192556	9.189325
6.949553	453.893455	9.194343
6.962730	452.604898	9.199360
6.942144	445.527656	9.204378
6.815702	464.210287	9.209395
6.945121	459.709679	9.214413
6.718299	465.867514	9.219431
7.013135	466.271223	9.224448
6.950246	463.473405	9.229466
7.091019	472.873453	9.234483
7.187695	469.013062	9.239501
7.042392	467.142847	9.244519
7.114127	461.991278	9.249536
6.946985	468.167198	9.254554
6.756353	473.406843	9.259571
7.363932	462.702202	9.264589
7.232238	463.181417	9.269607
7.313311	460.949647	9.274624
7.268050	455.527711	9.279642
6.775158	461.735123	9.284659
7.279137	455.347110	9.289677
7.164102	471.262101	9.294695
7.008310	466.940486	9.299712
6.973209	459.524270	9.304730
6.747518	474.177010	9.309747
7.000337	462.156674	9.314765
6.828042	466.250708	9.319783
7.021854	470.578177	9.324800
7.152931	467.872098	9.329818
6.874659	473.344684	9.334835
6.735534	466.581253	9.339853
6.848738	474.046101	9.344871
6.950826	456.083509	9.349888
7.277422	465.153594	9.354906
6.936308	461.042392	9.359923
7.216906	456.860135	9.364941
7.266669	479.256490	9.369959
7.274360	474.476646	9.374976
7.480140	470.243180	9.379994
6.904723	472.283210	9.385011
7.222245	467.345890	9.390029
7.190847	478.404961	9.395047
7.060222	466.738085	9.400064
6.926512	483.831228	9.405082
7.034260	489.992825	9.410099
7.470874	503.205511	9.415117
7.460100	497.053501	9.420135
7.509649	497.443919	9.425152
7.234342	490.447227	9.430170
7.408738	494.046565	9.435187
7.672416	482.640631	9.440205
7.110424	481.248443	9.445223
7.256930	470.797416	9.450240
7.330794	459.229207	9.455258
6.906816	470.925175	9.460275
7.427488	478.484762	9.465293
7.403868	492.114763	9.470311
7.645280	485.574795	9.475328
7.747743	466.565789	9.480346
7.125442	464.831673	9.485363
7.507411	461.145647	9.490381
7.388237	463.711434	9.495399
7.074625	468.175403	9.500416
7.414871	456.563076	9.505434
7.417340	470.224467	9.510451
7.338095	460.304845	9.515469
7.385759	469.931257	9.520487
7.112033	468.674268	9.525504
7.581169	468.343414	9.530522
7.133743	470.903126	9.535539
7.504652	480.943156	9.540557
7.955795	484.745723	9.545575
7.401422	473.243338	9.550592
7.206911	467.770093	9.555610
7.418981	473.306991	9.560627
7.530753	460.769625	9.565645
7.458863	466.504990	9.570663
7.084490	471.153375	9.575680
7.520711	479.060019	9.580698
7.695800	491.657092	9.585715
7.513515	477.230024	9.590733
7.424478	482.626075	9.595751
7.640545	489.284430	9.600768
7.610260	479.515629	9.605786
7.432127	477.461212	9.610803
7.384990	459.090295	9.615821
7.614446	483.266723	9.620839
7.470792	487.989856	9.625856
7.796892	486.487117	9.630874
7.696967	469.777326	9.635891
7.802869	458.318366	9.640909
7.631901	466.462816	9.645927
7.624577	466.408297	9.650944
7.673242	464.467749	9.655962
7.497425	466.880037	9.660979
7.370717	463.793517	9.665997
7.442626	459.494105	9.671015
7.399449	457.774401	9.676032
7.606435	468.939906	9.681050
7.618658	479.147160	9.686067
7.919008	489.064435	9.691085
7.680897	472.127628	9.696103
7.497868	464.091402	9.701120
7.833193	460.734376	9.706138
7.303807	472.626862	9.711155
7.722191	478.688312	9.716173
7.909266	477.591442	9.721191
7.528455	477.478393	9.726208
7.698669	468.909183	9.731226
7.507731	478.759638	9.736243
7.947855	478.679984	9.741261
7.842154	478.058870	9.746279
7.364188	469.785909	9.751296
7.830237	467.113334	9.756314
7.846358	484.812393	9.761331
7.716721	476.752577	9.766349
7.704637	473.222397	9.771367
7.749916	485.346827	9.776384
7.778470	472.085461	9.781402
7.816182	486.741230	9.786419
7.935098	477.576777	9.791437
7.711051	470.117780	9.796455
7.737354	472.869425	9.801472
7.873242	456.014895	9.806490
7.261415	476.054358	9.811507
7.705200	482.071954	9.816525
7.769802	492.194592	9.821543
7.636129	509.071561	9.826560
7.899892	493.549911	9.831578
7.812766	494.932992	9.836595
7.789180	496.548731	9.841613
7.966408	500.642481	9.846631
7.586379	495.354971	9.851648
8.173989	494.652051	9.856666
7.859822	494.692521	9.861683
7.857669	498.128753	9.866701
7.868074	492.266787	9.871719
7.659227	505.324088	9.876736
7.910344	491.258663	9.881754
7.799094	499.842087	9.886771
7.851009	502.708870	9.891789
8.111913	494.071815	9.896807
7.797845	500.343175	9.901824
7.815167	498.836454	9.906842
7.648327	497.695630	9.911859
7.808289	492.058996	9.916877
7.799626	506.634768	9.921895
7.896351	500.307741	9.926912
7.712791	493.874113	9.931930
8.204320	503.641325	9.936947
8.025163	507.284332	9.941965
8.078869	498.026040	9.946983
7.805242	502.360799	9.952000
8.126982	507.304310	9.957018
7.868983	506.146371	9.962035
7.810362	500.229484	9.967053
7.933786	508.960216	9.972071
7.835660	511.696316	9.977088
8.029378	527.014193	9.982106
8.369484	535.874847	9.987123
8.377774	509.770096	9.992141
8.063823	509.163616	9.997159
8.101821	509.827639	10.002176
8.116093	495.236406	10.007194
8.283527	508.746383	10.012211
8.399177	504.213201	10.017229
8.490139	498.323160	10.022247
8.048373	502.193876	10.027264
8.342243	508.689216	10.032282
8.240189	507.488286	10.037299
8.035585	500.557251	10.042317
8.200919	509.592903	10.047335
7.973107	512.143685	10.052352
8.123224	506.430047	10.057370
8.448345	519.333680	10.062387
8.195310	499.325821	10.067405
8.374161	504.311445	10.072423
8.153514	511.638707	10.077440
8.251049	497.544139	10.082458
8.027502	511.818686	10.087475
8.147406	509.451385	10.092493
8.003125	506.032199	10.097511
8.248626	514.034637	10.102528
8.027132	500.313490	10.107546
7.919273	511.575634	10.112563
7.860130	509.003816	10.117581
7.933988	497.604344	10.122599
8.358034	520.770823	10.127616
8.677226	523.355890	10.132634
8.322076	516.900029	10.137651
8.315508	510.755781	10.142669
8.402200	511.972864	10.147687
8.171948	504.024621	10.152704
8.172365	503.407028	10.157722
8.085601	512.377081	10.162739
8.247807	527.427977	10.167757
8.372801	527.559226	10.172775
8.425803	533.244357	10.177792
8.474464	527.482530	10.182810
8.614693	532.445319	10.187827
8.218183	529.157753	10.192845
8.387628	514.417261	10.197863
8.398838	527.116825	10.202880
8.423527	514.607287	10.207898
8.643276	500.853863	10.212915
7.903611	508.495293	10.217933
8.555581	514.918270	10.222951
8.477084	523.803122	10.227968
8.355482	521.752544	10.232986
8.526379	522.199763	10.238003
8.078279	532.636242	10.243021
8.461848	523.178669	10.248039
8.618295	540.415026	10.253056
8.384381	532.911280	10.258074
8.426608	530.995799	10.263091
8.902839	531.243968	10.268109
9.043539	517.946120	10.273127
8.501365	513.318242	10.278144
8.665018	502.251592	10.283162
8.463218	501.280488	10.288179
8.073038	500.843856	10.293197
8.611316	501.352090	10.298215
8.200184	513.361159	10.303232
8.368845	510.814871	10.308250
8.560591	515.563573	10.313267
8.669111	520.236875	10.318285
8.547365	522.711087	10.323303
8.755674	533.788743	10.328320
8.705393	525.923618	10.333338
8.717994	532.208612	10.338355
8.812530	531.591504	10.343373
8.859798	511.190569	10.348391
8.446766	508.530413	10.353408
8.229342	506.189533	10.358426
8.590196	511.688376	10.363443
8.740009	530.841472	10.368461
8.791075	527.019405	10.373479
8.680190	529.466238	10.378496
8.974333	527.415543	10.383514
8.908459	506.647661	10.388531
8.560454	505.316545	10.393549
8.466267	495.065383	10.398567
8.257731	505.098156	10.403584
8.418475	525.554781	10.408602
8.496025	522.918353	10.413619
8.630377	520.355985	10.418637
8.825316	518.033653	10.423655
8.965102	523.348016	10.428672
8.828200	533.471901	10.433690
8.938353	520.359279	10.438707
8.410736	525.897298	10.443725
8.908580	523.386452	10.448743
8.873649	524.326647	10.453760
8.708860	529.646767	10.458778
8.874610	522.261686	10.463795
8.654733	537.832728	10.468813
8.718294	524.488776	10.473831
8.658422	531.155356	10.478848
8.380654	539.690450	10.483866
8.711122	527.423322	10.488883
8.585731	538.770256	10.493901
8.790284	516.935437	10.498919
8.847571	530.963928	10.503936
8.570419	524.846874	10.508954
8.760277	520.812147	10.513971
8.612077	548.692374	10.518989
8.905229	555.161479	10.524007
9.114448	559.915278	10.529024
9.254603	556.696468	10.534042
8.867794	542.695184	10.539059
8.716568	543.417639	10.544077
8.894082	547.876636	10.549095
8.960020	554.700351	10.554112
8.769876	560.314279	10.559130
9.093642	561.553199	10.564147
8.755423	566.450015	10.569165
9.051100	573.559331	10.574183
9.320592	558.771856	10.579200
8.803326	567.926742	10.584218
9.136347	571.094652	10.589235
9.217886	566.562759	10.594253
9.198244	567.305883	10.599271
8.992815	537.536753	10.604288
8.786483	543.273109	10.609306
9.321187	549.039239	10.614323
9.046985	552.488852	10.619341
9.226256	548.544039	10.624359
8.895980	540.448266	10.629376
9.117445	562.379349	10.634394
9.402631	548.217905	10.639411
8.978546	534.389390	10.644429
9.253139	531.013749	10.649447
9.058656	529.324650	10.654464
8.942169	537.228685	10.659482
9.343011	534.621292	10.664499
9.102123	528.590056	10.669517
9.315151	529.327792	10.674535
9.369981	530.329615	10.679552
9.061684	535.670402	10.684570
8.894348	523.156968	10.689587
9.143353	540.525638	10.694605
9.181438	548.715194	10.699623
9.508803	547.692360	10.704640
8.868130	549.379281	10.709658
9.309809	541.365836	10.714675
9.341941	569.581875	10.719693
9.054494	566.299698	10.724711
9.346794	549.496269	10.729728
8.969651	564.397798	10.734746
9.121781	561.218928	10.739763
9.365549	576.793590	10.744781
9.314721	564.013575	10.749799
9.329892	564.011823	10.754816
9.198549	567.786187	10.759834
9.409421	562.060520	10.764851
9.355648	559.485346	10.769869
8.991826	566.007721	10.774887
9.266305	556.106339	10.779904
8.705042	573.541441	10.784922
9.165318	565.424733	10.789939
9.280827	565.730350	10.794957
8.787179	570.046971	10.799975
9.129841	563.231530	10.804992
9.106635	569.853689	10.810010
9.562530	576.829956	10.815027
9.928527	584.270894	10.820045
9.443080	583.495743	10.825063
9.665485	563.327654	10.830080
9.115373	567.693460	10.835098
9.362606	564.620305	10.840115
9.197926	572.008116	10.845133
9.378676	566.779748	10.850151
9.834135	577.447768	10.855168
9.232385	571.682309	10.860186
9.278909	570.753808	10.865203
9.491017	589.635219	10.870221
9.392829	579.065730	10.875239
9.406136	581.408994	10.880256
9.338037	585.706072	10.885274
9.739573	584.281293	10.890291
9.635475	588.408470	10.895309
9.573999	581.712750	10.900327
9.706746	578.711454	10.905344
9.704427	587.025204	10.910362
9.780130	580.328365	10.915379
9.667778	576.543624	10.920397
9.733370	579.265079	10.925415
9.530427	564.552425	10.930432
9.515968	564.620516	10.935450
9.661394	562.985554	10.940467
9.810990	576.248982	10.945485
9.272642	567.894823	10.950503
9.644288	562.946854	10.955520
9.609289	595.891691	10.960538
9.543356	582.231361	10.965555
9.870275	590.658289	10.970573
9.884816	591.610092	10.975591
9.627847	582.028559	10.980608
9.568720	585.013294	10.985626
9.847617	588.836676	10.990643
9.533445	592.070113	10.995661
9.630972	591.229620	11.000679
9.852113	597.381871	11.005696
9.793246	596.941951	11.010714
9.450723	587.780573	11.015731
9.877660	585.994777	11.020749
9.932734	593.965255	11.025767
9.882826	592.232773	11.030784
9.835612	597.106602	11.035802
9.900038	595.374907	11.040819
9.773862	591.319174	11.045837
9.529121	589.529341	11.050855
9.497386	592.007092	11.055872
9.578863	591.715697	11.060890
9.860050	585.529377	11.065907
9.970304	593.319608	11.070925
9.489234	586.870355	11.075943
9.579573	583.040899	11.080960
9.789357	584.708221	11.085978
10.102641	590.027196	11.090995
9.795199	597.578151	11.096013
9.766471	587.683064	11.101031
10.074622	594.878401	11.106048
9.698936	591.139831	11.111066
10.067307	592.112969	11.116083
9.676878	584.552107	11.121101
9.978407	593.006948	11.126119
10.181324	591.678856	11.131136
9.999469	589.994453	11.136154
10.166819	582.898785	11.141171
10.232856	577.448276	11.146189
9.996959	587.779463	11.151207
10.070516	585.771905	11.156224
10.150188	593.638534	11.161242
10.090985	587.168277	11.166259
10.062688	588.742194	11.171277
9.902873	591.151365	11.176295
9.947142	591.246653	11.181312
9.995233	589.699708	11.186330
9.745973	586.142569	11.191347
10.057955	592.636034	11.196365
9.935517	600.464131	11.201383
9.817894	589.671218	11.206400
10.024380	610.691249	11.211418
10.301081	612.738580	11.216435
10.432091	612.210009	11.221453
9.990203	602.699958	11.226471
10.199753	604.880506	11.231488
10.138625	600.688161	11.236506
10.065277	614.692852	11.241523
10.558770	611.602905	11.246541
10.448304	605.916647	11.251559
10.245123	596.188939	11.256576
10.141038	592.957639	11.261594
9.885719	592.040246	11.266611
10.399535	598.195499	11.271629
10.060794	597.180299	11.276647
10.391277	608.981766	11.281664
10.424341	608.030492	11.286682
10.156648	610.388609	11.291699
10.466372	594.144542	11.296717
10.239771	602.353955	11.301735
10.251286	597.204223	11.306752
10.149264	597.069308	11.311770
10.058382	608.129446	11.316787
10.103659	616.109426	11.321805
10.244832	624.588029	11.326823
10.479341	614.474458	11.331840
10.443229	624.380802	11.336858
10.285334	620.370749	11.341875
10.581234	618.054252	11.346893
10.181939	629.508218	11.351911
10.272709	613.860932	11.356928
10.442162	625.272963	11.361946
10.224202	629.961085	11.366963
10.436992	622.607052	11.371981
10.338830	622.524934	11.376999
10.326476	622.275418	11.382016
10.436261	622.481805	11.387034
10.331413	623.437792	11.392051
10.453481	625.451143	11.397069
10.369877	630.109485	11.402087
10.531187	624.029655	11.407104
10.371509	632.931135	11.412122
10.555066	637.169123	11.417139
10.788917	626.777460	11.422157
10.333463	631.758323	11.427175
10.644845	622.574280	11.432192
10.255256	618.683995	11.437210
10.307861	627.524018	11.442227
10.608740	617.185445	11.447245
10.115321	629.442801	11.452263
10.443103	642.465858	11.457280
10.575133	640.871283	11.462298
10.562474	651.771802	11.467315
10.593015	648.581124	11.472333
10.757716	651.718314	11.477351
11.006213	644.020642	11.482368
11.079420	646.052796	11.487386
10.498092	643.156307	11.492403
10.738284	627.144617	11.497421
10.595783	626.926645	11.502439
10.483424	617.090529	11.507456
10.618727	633.985573	11.512474
10.853021	648.284861	11.517491
11.090404	640.039626	11.522509
10.575779	640.559789	11.527527
11.220463	629.003005	11.532544
10.740777	624.759078	11.537562
10.327976	631.154365	11.542579
10.665076	622.242690	11.547597
10.628079	645.134633	11.552615
10.796937	642.453474	11.557632
10.965375	645.354069	11.562650
10.799875	653.662839	11.567667
11.153120	650.598817	11.572685
11.257783	641.179192	11.577703
11.052792	625.259180	11.582720
11.012254	622.092063	11.587738
10.807723	617.279837	11.592755
10.763806	619.709812	11.597773
10.732749	619.883186	11.602791
10.378266	617.515243	11.607808
10.905003	629.936134	11.612826
10.817217	642.047546	11.617843
11.130361	653.483480	11.622861
10.356500	650.712292	11.627879
10.544035	657.217887	11.632896
10.838105	662.139943	11.637914
10.995121	651.720515	11.642931
10.737732	655.531967	11.647949
10.727344	658.365580	11.652967
11.070824	654.465145	11.657984
11.371665	658.859511	11.663002
10.595242	658.691584	11.668019
10.808585	655.126668	11.673037
10.809440	652.409898	11.678055
11.059273	667.253379	11.683072
11.303748	663.735274	11.688090
11.018752	658.012202	11.693107
11.084739	656.945761	11.698125
11.268141	653.763673	11.703143
11.240303	658.630285	11.708160
11.198188	654.342872	11.713178
10.694450	658.943807	11.718195
11.288824	666.030570	11.723213
11.172207	667.271226	11.728231
11.109166	667.093163	11.733248
11.196247	657.515245	11.738266
10.835456	674.115520	11.743283
11.296331	680.252198	11.748301
11.388987	685.674582	11.753319
11.366755	693.054755	11.758336
11.328265	677.211976	11.763354
11.473385	672.374425	11.768371
11.348616	655.658993	11.773389
11.443755	659.233976	11.778407
11.166169	656.959598	11.783424
10.962532	646.644844	11.788442
11.505275	653.319743	11.793459
11.012415	643.672154	11.798477
11.251568	655.555862	11.803495
11.342830	668.993446	11.808512
11.650931	675.309276	11.813530
11.218812	657.214792	11.818547
11.187023	654.350887	11.823565
11.189149	667.892651	11.828583
11.232854	681.284966	11.833600
11.634291	669.807713	11.838618
11.488135	686.932167	11.843635
11.815874	674.022978	11.848653
11.376245	652.790191	11.853671
11.122812	658.903101	11.858688
11.617227	670.851112	11.863706
11.279337	673.327708	11.868723
11.386117	683.831124	11.873741
11.445993	685.164540	11.878759
11.412893	695.770986	11.883776
11.697496	671.811511	11.888794
11.524208	682.029678	11.893811
11.660182	676.853152	11.898829
11.384967	675.610267	11.903847
11.088105	682.123692	11.908864
11.564345	677.901664	11.913882
11.458798	686.138057	11.918899
11.344696	679.419107	11.923917
11.461558	679.432925	11.928935
11.246560	678.513980	11.933952
11.436855	679.084451	11.938970
11.503033	685.704878	11.943987
11.638218	676.459485	11.949005
11.717572	680.663043	11.954023
11.457444	687.188407	11.959040
11.559120	671.288620	11.964058
11.655177	681.608902	11.969075
11.537722	674.228628	11.974093
11.593350	689.175863	11.979111
11.555610	703.463179	11.984128
11.891565	699.320322	11.989146
11.929414	708.346850	11.994163
11.763651	695.838821	11.999181
11.941307	684.454530	12.004199
11.953302	689.265268	12.009216
11.916005	681.823919	12.014234
11.515895	679.195842	12.019251
11.812265	671.384655	12.024269
11.508051	678.667944	12.029287
11.679429	698.489405	12.034304
12.116632	694.394765	12.039322
11.696126	713.896226	12.044339
11.980369	705.635241	12.049357
12.375247	708.884869	12.054375
11.737811	695.125514	12.059392
11.932496	683.940930	12.064410
11.751018	690.137907	12.069427
11.774820	683.279948	12.074445
12.294334	700.749049	12.079463
12.094579	703.852008	12.084480
12.005184	678.841254	12.089498
11.915965	682.276367	12.094515
11.779091	679.912210	12.099533
11.991944	680.760493	12.104551
11.763357	692.933296	12.109568
12.381185	684.109617	12.114586
11.765409	676.613502	12.119603
11.936933	682.176858	12.124621
11.957601	693.306893	12.129639
11.777831	701.064217	12.134656
12.162884	699.578384	12.139674
12.158559	711.728411	12.144691
11.967782	706.970959	12.149709
12.112063	702.448635	12.154727
12.096670	705.208393	12.159744
12.095960	704.862186	12.164762
12.282297	709.516781	12.169779
12.280953	713.163517	12.174797
12.246962	703.743938	12.179815
12.040887	713.552172	12.184832
12.194765	713.151289	12.189850
12.445802	707.349161	12.194867
12.256090	709.113415	12.199885
12.198257	700.246590	12.204903
12.045199	704.059806	12.209920
12.051615	702.329025	12.214938
12.429079	705.003688	12.219955
12.320374	707.814194	12.224973
12.296131	708.829982	12.229991
12.325608	714.908265	12.235008
12.615032	695.928698	12.240026
12.348318	696.000295	12.245043
12.501770	692.258689	12.250061
12.133673	685.787281	12.255079
11.897255	684.303875	12.260096
12.094319	698.705209	12.265114
12.234191	699.268269	12.270131
12.197443	706.946164	12.275149
12.384864	697.994921	12.280167
12.213563	713.975652	12.285184
12.604625	714.234062	12.290202
12.545505	711.145671	12.295219
12.019320	710.032626	12.300237
12.504144	698.710830	12.305255
12.007830	708.647914	12.310272
12.001572	710.328220	12.315290
12.014377	715.188036	12.320307
12.333138	734.865231	12.325325
12.469423	741.500765	12.330343
12.270978	733.844236	12.335360
12.650659	752.462373	12.340378
12.776981	741.334509	12.345395
12.489019	751.904976	12.350413
12.667146	746.827444	12.355431
12.732381	739.564066	12.360448
12.892892	747.617574	12.365466
12.680552	742.510297	12.370483
12.620725	732.197994	12.375501
12.503093	741.833687	12.380519
12.502018	746.986696	12.385536
12.808098	741.373749	12.390554
13.135935	733.424284	12.395571
12.688917	730.242443	12.400589
12.621744	710.960438	12.405607
12.537048	710.414470	12.410624
12.201789	722.620768	12.415642
12.842707	736.080548	12.420659
12.596826	738.883125	12.425677
13.055448	737.911508	12.430695
12.500169	746.902439	12.435712
12.391322	747.375426	12.440730
12.726446	746.408571	12.445747
12.661840	750.674907	12.450765
12.955564	750.385534	12.455783
12.875882	740.006736	12.460800
12.866017	747.949942	12.465818
13.021230	736.754425	12.470835
12.779075	741.727431	12.475853
13.265933	731.473971	12.480871
12.821596	743.210903	12.485888
12.871666	747.120360	12.490906
12.863655	742.523013	12.495923
12.973369	743.477795	12.500941
13.005015	751.534297	12.505959
12.611297	742.088822	12.510976
12.923136	744.977842	12.515994
13.250177	741.743165	12.521011
12.747518	745.978170	12.526029
13.056026	747.694537	12.531047
12.795473	736.995107	12.536064
12.673822	742.991015	12.541082
13.273545	742.779396	12.546099
13.143436	739.734909	12.551117
12.827062	735.450580	12.556135
12.911175	738.505160	12.561152
12.930586	738.300776	12.566170
12.898247	734.513697	12.571187
12.781756	738.273642	12.576205
13.033722	733.937018	12.581223
13.027930	740.175736	12.586240
13.372325	758.343499	12.591258
13.346274	739.126106	12.596275
12.938876	741.952915	12.601293
12.866427	732.261478	12.606311
12.797647	758.165258	12.611328
12.915884	756.893855	12.616346
13.124696	767.853311	12.621363
12.933160	768.871360	12.626381
13.275083	763.506075	12.631399
13.087622	777.012743	12.636416
13.399670	774.800819	12.641434
13.482070	783.641322	12.646451
13.039749	779.243862	12.651469
13.275811	772.206029	12.656487
13.397045	774.369215	12.661504
13.068476	774.045992	12.666522
13.386583	773.660086	12.671539
13.035402	769.472722	12.676557
13.268139	766.674805	12.681575
13.196687	776.847570	12.686592
13.127311	771.750313	12.691610
13.586644	784.857735	12.696627
13.617443	797.547593	12.701645
13.722264	777.681771	12.706663
13.694933	765.988053	12.711680
13.618976	769.745146	12.716698
13.584497	766.169691	12.721715
13.615886	778.603874	12.726733
13.624169	763.994580	12.731751
13.496984	767.526028	12.736768
13.447557	773.040808	12.741786
13.794064	761.688389	12.746803
13.652900	767.258576	12.751821
13.367801	772.055554	12.756839
13.735337	766.647263	12.761856
13.601102	771.449915	12.766874
13.799101	764.339356	12.771891
13.805504	772.517734	12.776909
13.766600	770.861253	12.781927
13.708574	769.304568	12.786944
13.607795	772.546865	12.791962
13.936647	762.423412	12.796979
13.843239	772.841490	12.801997
13.545495	758.513144	12.807015
13.651752	758.484038	12.812032
13.581199	770.165717	12.817050
13.641370	759.728073	12.822067
13.310016	762.984460	12.827085
13.484476	757.879977	12.832103
13.474159	756.777821	12.837120
13.255323	767.891890	12.842138
13.612031	786.706151	12.847155
13.829286	791.735021	12.852173
13.801492	799.246159	12.857191
14.009521	795.124023	12.862208
13.627442	814.299634	12.867226
13.999140	798.438838	12.872243
14.028563	792.954351	12.877261
14.162810	801.403788	12.882279
14.139500	785.691239	12.887296
13.633746	785.997676	12.892314
13.908084	783.178711	12.897331
14.020896	795.232787	12.902349
14.091889	795.993516	12.907367
14.279939	800.129646	12.912384
13.716142	780.067185	12.917402
14.179480	777.857321	12.922419
13.659766	791.339691	12.927437
13.950466	784.466118	12.932455
14.057873	788.757474	12.937472
13.985774	797.677345	12.942490
14.074900	792.021014	12.947507
14.072267	804.478258	12.952525
13.757408	796.938949	12.957543
13.998610	807.158178	12.962560
14.014636	812.561190	12.967578
14.213731	790.391416	12.972595
14.200982	800.949796	12.977613
14.075132	798.150907	12.982631
14.134357	806.852661	12.987648
14.088179	803.136146	12.992666
14.001286	812.936458	12.997683
14.175414	801.636015	13.002701
13.983019	799.486981	13.007719
14.362755	798.087829	13.012736
13.898620	807.276882	13.017754
14.138344	799.956497	13.022771
14.182027	801.897210	13.027789
13.997528	806.926938	13.032807
14.628849	829.034820	13.037824
14.269763	826.452094	13.042842
14.648334	822.671680	13.047859
14.588157	818.789494	13.052877
14.355529	807.252089	13.057895
14.634272	808.447889	13.062912
14.347808	789.947260	13.067930
14.624872	797.515675	13.072947
14.500236	803.246499	13.077965
14.370555	803.700002	13.082983
14.720041	795.015469	13.088000
14.223599	805.776105	13.093018
14.401161	804.268362	13.098035
14.580960	800.487441	13.103053
14.583307	816.407403	13.108071
14.554310	804.366357	13.113088
14.549582	806.757706	13.118106
14.329207	800.263412	13.123123
14.606639	795.629802	13.128141
14.185148	802.896118	13.133159
14.523292	803.739547	13.138176
14.398403	809.055432	13.143194
14.594031	815.269457	13.148211
14.701245	835.964926	13.153229
14.688154	827.898950	13.158247
14.833283	833.578415	13.163264
14.698923	836.654652	13.168282
14.911861	827.489215	13.173299
14.891915	815.612088	13.178317
14.888286	810.756268	13.183335
14.640532	795.495584	13.188352
14.548689	797.640452	13.193370
14.754467	808.096497	13.198387
14.583937	817.641588	13.203405
14.737854	817.185195	13.208423
14.812406	830.739441	13.213440
14.591563	835.959501	13.218458
14.842039	835.000822	13.223475
14.696900	830.322389	13.228493
14.934799	826.087061	13.233511
14.889517	816.228021	13.238528
14.286926	824.793334	13.243546
14.558149	829.407565	13.248563
15.039604	827.187221	13.253581
14.993039	825.971092	13.258599
14.940491	823.931006	13.263616
14.778542	831.799799	13.268634
14.906166	833.854673	13.273651
15.157748	831.857912	13.278669
14.824249	823.365743	13.283687
15.375890	830.774352	13.288704
15.126853	830.697779	13.293722
15.187294	835.164497	13.298739
15.082273	837.494880	13.303757
15.271819	839.207004	13.308775
15.267190	823.583536	13.313792
15.017461	830.616794	13.318810
15.093735	834.861841	13.323827
15.262807	829.469104	13.328845
14.897521	841.064233	13.333863
15.148549	827.784198	13.338880
15.087299	830.314198	13.343898
15.198664	833.873551	13.348915
15.026930	824.665602	13.353933
14.693235	833.061111	13.358951
15.178764	833.920631	13.363968
15.046639	837.278829	13.368986
15.419195	850.589787	13.374003
15.410542	850.155634	13.379021
15.248596	851.319262	13.384039
15.534467	839.962931	13.389056
15.053832	833.310979	13.394074
15.341941	858.442794	13.399091
15.557335	857.041568	13.404109
15.270848	854.844799	13.409127
15.428826	854.616826	13.414144
15.373489	851.696649	13.419162
15.406330	862.728257	13.424179
15.974859	854.122630	13.429197
15.317572	844.102257	13.434215
15.275639	828.051466	13.439232
15.246851	845.204034	13.444250
15.568211	858.399860	13.449267
15.671729	848.325496	13.454285
15.544018	861.107533	13.459303
15.817493	856.728548	13.464320
15.527811	847.087994	13.469338
15.067055	836.956717	13.474355
15.625037	845.605594	13.479373
15.469308	863.350709	13.484391
15.770002	861.759237	13.489408
15.568952	860.597863	13.494426
15.696113	862.716388	13.499443
15.678097	860.835324	13.504461
15.644552	853.929985	13.509479
16.052582	854.650175	13.514496
16.032657	845.133714	13.519514
15.562474	837.479134	13.524531
15.808688	826.868305	13.529549
15.627213	825.080387	13.534567
15.756709	827.009875	13.539584
15.595151	823.119938	13.544602
15.595926	849.237631	13.549619
15.646414	853.791416	13.554637
15.580572	857.536034	13.559655
15.637865	850.182201	13.564672
15.609243	853.205344	13.569690
15.765189	864.510947	13.574707
16.033519	854.528908	13.579725
15.803780	858.710083	13.584743
15.927428	862.641754	13.589760
16.028397	866.958403	13.594778
15.950018	858.911959	13.599795
15.946000	855.921008	13.604813
15.789524	866.184640	13.609831
15.703905	858.898310	13.614848
15.724663	861.598883	13.619866
15.496455	859.312871	13.624883
15.914449	861.207382	13.629901
15.975327	881.443233	13.634919
16.108990	884.079295	13.639936
16.029946	885.653362	13.644954
16.006518	891.494243	13.649971
16.571480	887.498202	13.654989
16.339207	876.694511	13.660007
16.417776	885.439857	13.665024
16.260330	864.151878	13.670042
15.979768	866.852945	13.675059
16.320990	874.044031	13.680077
16.068205	868.478224	13.685095
16.153343	884.976889	13.690112
16.392895	884.939434	13.695130
16.323022	880.434636	13.700147
16.478861	881.216480	13.705165
16.100661	872.972572	13.710183
16.125834	876.481328	13.715200
16.491758	879.743945	13.720218
16.456103	886.563833	13.725235
16.696984	881.163246	13.730253
16.204036	868.437245	13.735271
16.207681	864.684928	13.740288
16.230312	873.001598	13.745306
16.304227	880.503447	13.750323
16.470278	879.848626	13.755341
16.546895	880.704968	13.760359
16.735664	877.214620	13.765376
16.704594	875.810232	13.770394
16.639026	882.171464	13.775411
16.774189	862.914384	13.780429
16.382447	860.033462	13.785447
16.162222	863.197798	13.790464
16.438338	863.592508	13.795482
16.453508	879.386423	13.800499
16.426181	876.937609	13.805517
16.719713	886.996794	13.810535
16.398964	887.417319	13.815552
16.688823	885.972491	13.820570
16.678756	892.784906	13.825587
16.473119	883.737319	13.830605
16.283188	894.599109	13.835623
16.590041	872.989553	13.840640
16.399067	875.064116	13.845658
16.646111	870.854917	13.850675
16.977887	875.291666	13.855693
16.748016	885.413925	13.860711
16.391785	877.381699	13.865728
16.593719	879.308277	13.870746
16.430487	884.334220	13.875763
16.462212	897.375322	13.880781
16.971440	906.362152	13.885799
16.953484	912.525405	13.890816
16.970853	918.286830	13.895834
16.731389	912.795268	13.900851
16.867635	904.179667	13.905869
16.996131	915.284663	13.910887
17.145904	916.323962	13.915904
17.180589	911.481165	13.920922
16.998072	922.436319	13.925939
17.202819	904.309119	13.930957
17.044386	905.571957	13.935975
16.975158	893.389484	13.940992
17.100317	897.745346	13.946010
16.580333	901.097194	13.951027
17.135037	907.380732	13.956045
16.883970	911.493511	13.961063
17.082791	904.098156	13.966080
16.832645	903.783620	13.971098
16.917336	908.358535	13.976115
17.063647	910.017981	13.981133
16.689892	910.670159	13.986151
16.739569	906.243217	13.991168
17.057211	917.100559	13.996186
16.945512	913.276952	14.001203
17.531399	915.864660	14.006221
17.514050	926.692540	14.011239
17.116630	920.289056	14.016256
17.645819	929.981727	14.021274
16.960227	921.362190	14.026291
17.463257	920.120770	14.031309
17.252203	929.646451	14.036327
17.600622	934.392912	14.041344
17.293943	932.155874	14.046362
17.328820	930.532450	14.051379
17.477440	927.417066	14.056397
17.230631	923.480769	14.061415
17.472241	936.917656	14.066432
17.466367	938.495579	14.071450
17.345019	932.700486	14.076467
17.742604	928.354701	14.081485
17.639129	927.383557	14.086503
17.516147	928.850245	14.091520
17.674053	924.586385	14.096538
17.442373	927.718086	14.101555
17.733399	926.422051	14.106573
17.802673	935.691802	14.111591
17.426902	941.950214	14.116608
17.826926	923.859508	14.121626
17.196845	931.789279	14.126643
17.513819	943.339934	14.131661
17.552733	931.134149	14.136679
17.377086	933.593028	14.141696
18.139639	920.709694	14.146714
17.640234	939.774754	14.151731
17.726944	929.646924	14.156749
17.725373	933.316876	14.161767
17.352522	933.077134	14.166784
17.694206	934.466936	14.171802
17.450457	929.563373	14.176819
17.553277	932.512360	14.181837
17.445374	925.490067	14.186855
17.774695	950.716582	14.191872
18.116874	960.929855	14.196890
17.853074	966.784310	14.201907
18.335412	955.582106	14.206925
18.139229	941.937076	14.211943
17.681585	932.823349	14.216960
18.200121	919.894627	14.221978
17.692583	931.342692	14.226995
18.201339	933.391574	14.232013
18.385141	930.411394	14.237031
17.847715	918.230796	14.242048
18.209158	925.257176	14.247066
18.069149	935.931446	14.252083
18.176098	920.662013	14.257101
17.870622	922.981349	14.262119
17.659197	927.805170	14.267136
18.154723	934.267268	14.272154
18.349038	957.152842	14.277171
18.212536	953.898382	14.282189
18.268610	963.708524	14.287207
18.067458	964.132216	14.292224
18.224276	968.537187	14.297242
18.183784	962.743973	14.302259
18.347729	972.621418	14.307277
18.412733	963.317974	14.312295
18.260573	958.264940	14.317312
18.751934	965.297030	14.322330
18.368591	969.624267	14.327347
18.374578	969.341405	14.332365
18.528542	962.756248	14.337383
18.159221	961.472404	14.342400
18.389187	952.833514	14.347418
18.260842	955.086583	14.352435
18.129897	966.064932	14.357453
18.223974	958.015326	14.362471
18.346864	963.736992	14.367488
18.660877	961.112977	14.372506
18.379473	964.446570	14.377523
18.348781	969.968362	14.382541
18.494230	958.417962	14.387559
18.402042	957.572586	14.392576
18.304984	957.566747	14.397594
18.537837	962.419798	14.402611
18.634450	960.418124	14.407629
18.772705	949.717885	14.412647
18.629483	958.240718	14.417664
18.676700	966.794278	14.422682
18.730954	969.950278	14.427699
18.712164	974.505510	14.432717
18.959757	968.990319	14.437735
18.638356	978.368251	14.442752
18.961750	969.668349	14.447770
18.632513	973.531115	14.452787
18.536699	985.837103	14.457805
18.793429	988.810460	14.462823
18.573340	1004.207924	14.467840
18.741904	989.540044	14.472858
19.096779	985.624063	14.477875
18.866711	988.862185	14.482893
19.001765	986.842345	14.487911
18.993558	985.731460	14.492928
19.036640	980.132070	14.497946
18.955895	987.152924	14.502963
19.150129	989.423840	14.507981
19.271868	989.073923	14.512999
18.961721	1000.701391	14.518016
19.537438	989.995847	14.523034
19.202833	984.442633	14.528051
18.935089	978.085301	14.533069
19.198975	975.480688	14.538087
18.865071	976.844465	14.543104
19.072749	971.825646	14.548122
19.379595	993.623573	14.553139
19.290407	995.889071	14.558157
19.212675	979.521652	14.563175
18.924830	982.085285	14.568192
19.355707	992.546179	14.573210
19.792602	980.811304	14.578227
18.986329	980.832425	14.583245
19.594869	980.853067	14.588263
19.397239	970.036205	14.593280
19.062487	967.897386	14.598298
18.603838	966.203574	14.603315
18.769414	982.384478	14.608333
19.438385	987.672171	14.613351
18.969812	997.982349	14.618368
18.999362	991.828496	14.623386
19.159199	995.647645	14.628403
19.055158	1016.750251	14.633421
19.604686	1010.468736	14.638439
19.580676	1025.965490	14.643456
19.748323	1025.609954	14.648474
19.607232	1027.871143	14.653491
19.410145	1033.619339	14.658509
19.811787	1020.422203	14.663527
19.514339	1022.220336	14.668544
19.736457	1025.634484	14.673562
19.694032	1024.523838	14.678579
19.839686	1026.703985	14.683597
19.790992	1018.980940	14.688615
20.060188	1019.819439	14.693632
19.482969	996.137782	14.698650
19.668563	997.781002	14.703667
19.736570	1007.696564	14.708685
19.998535	1016.299984	14.713703
19.728161	1011.214410	14.718720
19.608313	1013.673527	14.723738
19.785176	1014.667812	14.728755
19.820265	1025.963491	14.733773
19.919354	1022.444040	14.738791
19.728860	1023.308711	14.743808
19.788378	1018.327942	14.748826
19.686751	1019.660915	14.753843
19.655907	1017.115334	14.758861
19.564769	1018.985654	14.763879
19.820888	1015.708517	14.768896
19.491832	1011.798582	14.773914
19.823079	1026.775683	14.778931
19.850193	1048.080439	14.783949
20.062725	1048.312857	14.788967
19.934057	1049.618024	14.793984
19.921134	1047.517825	14.799002
20.261546	1051.799878	14.804019
20.306749	1050.165584	14.809037
20.465121	1050.303033	14.814055
20.470709	1043.605476	14.819072
20.394619	1044.849206	14.824090
20.685416	1025.561972	14.829107
20.279278	1018.957263	14.834125
20.497435	1012.900460	14.839143
20.118359	1020.488651	14.844160
19.949080	1013.455303	14.849178
20.246907	1016.854772	14.854195
20.073311	1013.491785	14.859213
20.183404	1024.246615	14.864231
20.095189	1035.884669	14.869248
20.560033	1041.147364	14.874266
20.669888	1047.957842	14.879283
20.095989	1046.201289	14.884301
20.453526	1038.256208	14.889319
20.070907	1039.886166	14.894336
20.226091	1042.302101	14.899354
20.591275	1041.276038	14.904371
20.393067	1047.445219	14.909389
20.463779	1041.298616	14.914407
20.718278	1043.348396	14.919424
20.635566	1039.471452	14.924442
20.822341	1045.708683	14.929459
20.411894	1052.013316	14.934477
20.316566	1045.076769	14.939495
20.538586	1049.756078	14.944512
20.565224	1045.621340	14.949530
20.638930	1045.946373	14.954547
20.494041	1056.194636	14.959565
20.737443	1071.550115	14.964583
20.492950	1071.914349	14.969600
20.532983	1086.248902	14.974618
20.973353	1087.597021	14.979635
21.138087	1087.829269	14.984653
20.890054	1088.770370	14.989671
20.921763	1081.898626	14.994688
20.804916	1095.122295	14.999706
21.182545	1082.102274	15.004723
21.137445	1078.823335	15.009741
21.004085	1085.640956	15.014759
21.282949	1086.828591	15.019776
20.875638	1069.875391	15.024794
20.896387	1067.644056	15.029811
21.124616	1080.147216	15.034829
21.153625	1071.304402	15.039847
21.146188	1074.610851	15.044864
21.191984	1078.298793	15.049882
21.439471	1066.567993	15.054899
20.939230	1055.459895	15.059917
21.075422	1045.495830	15.064935
21.408479	1067.306653	15.069952
20.940180	1076.078120	15.074970
21.190261	1065.680330	15.079987
21.203889	1088.596746	15.085005
21.124267	1080.355246	15.090023
21.230199	1075.562227	15.095040
21.456427	1079.132571	15.100058
21.571164	1069.931358	15.105075
21.267177	1083.068245	15.110093
21.117810	1079.362319	15.115111
21.568200	1071.913405	15.120128
21.577623	1086.683260	15.125146
21.494207	1084.030233	15.130163
21.174947	1093.029204	15.135181
21.140816	1080.947950	15.140199
21.486621	1076.105254	15.145216
21.188412	1082.403161	15.150234
21.453411	1077.957218	15.155251
20.942860	1087.256453	15.160269
20.900112	1082.807044	15.165287
21.278332	1098.083586	15.170304
21.563290	1109.819648	15.175322
21.725571	1111.535324	15.180339
21.522111	1109.866538	15.185357
21.590383	1104.546752	15.190375
21.886049	1108.833263	15.195392
21.535498	1116.905683	15.200410
21.401325	1105.493000	15.205427
21.466188	1115.706051	15.210445
21.613255	1109.206505	15.215463
21.811742	1114.769302	15.220480
21.814241	1110.199237	15.225498
21.808911	1102.337116	15.230515
21.224360	1113.843900	15.235533
21.432792	1124.119437	15.240551
21.792740	1126.882391	15.245568
22.045554	1144.570059	15.250586
22.171347	1138.078740	15.255603
22.185162	1143.323500	15.260621
21.809010	1141.530124	15.265639
21.830699	1139.151600	15.270656
22.144398	1147.063880	15.275674
22.410075	1131.862086	15.280691
22.313601	1137.508078	15.285709
22.100615	1145.805968	15.290727
22.343818	1138.972858	15.295744
22.215378	1142.802385	15.300762
21.956594	1136.421069	15.305779
22.017857	1143.156365	15.310797
22.118368	1124.084675	15.315815
22.460314	1135.779061	15.320832
22.099307	1139.433275	15.325850
22.420261	1128.058338	15.330867
22.344794	1141.278948	15.335885
22.440866	1134.833874	15.340903
22.376007	1137.246430	15.345920
22.222021	1144.367044	15.350938
22.491088	1139.024691	15.355955
22.588055	1136.808305	15.360973
22.448434	1140.987457	15.365991
22.653285	1138.663690	15.371008
22.503984	1144.906705	15.376026
22.387770	1143.771833	15.381043
22.582332	1136.936921	15.386061
22.553934	1139.778420	15.391079
22.879940	1141.328484	15.396096
22.357164	1139.313512	15.401114
22.272963	1133.382009	15.406131
22.367715	1138.190627	15.411149
22.299033	1137.781245	15.416167
22.568594	1133.923807	15.421184
22.789807	1131.695156	15.426202
22.645506	1132.116837	15.431219
22.523046	1142.996977	15.436237
22.477770	1149.077551	15.441255
22.970107	1155.606795	15.446272
22.495635	1159.526969	15.451290
22.791088	1166.051948	15.456307
23.048549	1161.866437	15.461325
22.734698	1165.535893	15.466343
22.824001	1162.648634	15.471360
22.713152	1161.200720	15.476378
22.860546	1165.852050	15.481395
22.985715	1167.965928	15.486413
22.687521	1169.290262	15.491431
22.797734	1162.478135	15.496448
22.727203	1169.495613	15.501466
22.911332	1164.908901	15.506483
23.181651	1160.703355	15.511501
22.967154	1165.385555	15.516519
23.182559	1158.876861	15.521536
22.796831	1168.239558	15.526554
22.938494	1181.096224	15.531571
23.318414	1189.496124	15.536589
23.292252	1194.691809	15.541607
23.675569	1189.332724	15.546624
23.260967	1179.748523	15.551642
23.401333	1166.174035	15.556659
23.462875	1161.320227	15.561677
22.984797	1171.501010	15.566695
23.880836	1165.381132	15.571712
23.321987	1165.213355	15.576730
23.180358	1165.255130	15.581747
23.506339	1158.071969	15.586765
23.229330	1166.858719	15.591783
23.427391	1179.290973	15.596800
23.567704	1196.746743	15.601818
23.846648	1186.491716	15.606835
23.617094	1187.666542	15.611853
23.355196	1176.109783	15.616871
23.127970	1178.224230	15.621888
23.152593	1192.936172	15.626906
23.355283	1195.961702	15.631923
23.959531	1192.139281	15.636941
23.663138	1203.813832	15.641959
23.513092	1195.868902	15.646976
23.582238	1199.913980	15.651994
23.794194	1194.484605	15.657011
23.678510	1192.704273	15.662029
23.683076	1198.721126	15.667047
23.772177	1200.287712	15.672064
23.760624	1206.161586	15.677082
23.467627	1195.144119	15.682099
23.999941	1199.811167	15.687117
23.956069	1206.954551	15.692135
23.994117	1195.742045	15.697152
23.714198	1210.690915	15.702170
23.834473	1210.011170	15.707187
24.143341	1219.664955	15.712205
24.236937	1225.429742	15.717223
24.443603	1226.739341	15.722240
23.713616	1208.454097	15.727258
23.688811	1214.784619	15.732275
24.151007	1212.908001	15.737293
23.762944	1218.626614	15.742311
24.070275	1216.729531	15.747328
24.020570	1214.205732	15.752346
24.156106	1218.798023	15.757363
24.480918	1216.739021	15.762381
23.971845	1224.583600	15.767399
24.149456	1218.389344	15.772416
24.064890	1217.316352	15.777434
23.972528	1221.197408	15.782451
24.406130	1217.659045	15.787469
24.129202	1232.702113	15.792487
24.286665	1245.549923	15.797504
24.723505	1253.696987	15.802522
24.941290	1248.370748	15.807539
24.850469	1236.357196	15.812557
24.444726	1225.788980	15.817575
24.828594	1225.978916	15.822592
24.571111	1220.811135	15.827610
24.594202	1214.395015	15.832627
24.623634	1213.525196	15.837645
24.330277	1225.544287	15.842663
24.613063	1217.765182	15.847680
24.603320	1219.621092	15.852698
24.539862	1212.889209	15.857715
24.593964	1218.191107	15.862733
24.465066	1244.726802	15.867751
24.624004	1251.352121	15.872768
24.876008	1249.534442	15.877786
24.657248	1258.440731	15.882803
25.041177	1253.912496	15.887821
24.933763	1252.042811	15.892839
24.860335	1249.888814	15.897856
24.994327	1250.919526	15.902874
24.767489	1254.835212	15.907891
25.336358	1246.874979	15.912909
24.861166	1241.028319	15.917927
24.974168	1248.179061	15.922944
25.123485	1249.122016	15.927962
24.876349	1251.726892	15.932979
25.175775	1257.503339	15.937997
24.784129	1249.184985	15.943015
25.220829	1244.944049	15.948032
25.048210	1237.379737	15.953050
24.747905	1243.652469	15.958067
25.266518	1238.934094	15.963085
24.944970	1245.965533	15.968103
24.984012	1245.850306	15.973120
25.171620	1241.420255	15.978138
24.852516	1246.663185	15.983155
25.316094	1264.073483	15.988173
25.155393	1271.793007	15.993191
25.325492	1275.546858	15.998208
25.112790	1275.271885	16.003226
24.896672	1273.474287	16.008243
25.187869	1269.863595	16.013261
25.324336	1281.342677	16.018279
25.453414	1269.719859	16.023296
25.633520	1269.957247	16.028314
25.132642	1280.693752	16.033331
25.548264	1290.045140	16.038349
25.658166	1301.254654	16.043367
25.771132	1309.257268	16.048384
26.049086	1306.889904	16.053402
26.029615	1290.461452	16.058419
25.758324	1279.252964	16.063437
25.839768	1279.023069	16.068455
25.766242	1272.230038	16.073472
26.089172	1270.633867	16.078490
25.947308	1267.358282	16.083507
25.880714	1263.781917	16.088525
25.833754	1270.339121	16.093543
25.749293	1263.045223	16.098560
25.806503	1273.211225	16.103578
25.773966	1268.604193	16.108595
25.737754	1268.287655	16.113613
25.783629	1288.608693	16.118631
26.094918	1291.089409	16.123648
26.227519	1306.353804	16.128666
26.047731	1304.864717	16.133683
26.414351	1298.808461	16.138701
26.267614	1307.225588	16.143719
26.092444	1284.540957	16.148736
25.987720	1269.821039	16.153754
25.879398	1291.659851	16.158771
26.145610	1286.026036	16.163789
26.209908	1297.417859	16.168807
26.041009	1290.597280	16.173824
26.207668	1297.170170	16.178842
26.039250	1295.843354	16.183859
26.383275	1296.902736	16.188877
26.271381	1303.574211	16.193895
26.268556	1290.001627	16.198912
26.121212	1301.411895	16.203930
26.195030	1300.133223	16.208947
26.326674	1301.373940	16.213965
26.151966	1298.249422	16.218983
26.315990	1309.135085	16.224000
26.689257	1309.121688	16.229018
26.688309	1321.259829	16.234035
26.652675	1313.367770	16.239053
26.782143	1313.917023	16.244071
26.488357	1320.678595	16.249088
26.684257	1312.461311	16.254106
26.476647	1319.783553	16.259123
26.943458	1324.644114	16.264141
26.775741	1319.700996	16.269159
26.737901	1317.543667	16.274176
27.080478	1314.578311	16.279194
26.743741	1324.836609	16.284211
26.985143	1319.624732	16.289229
26.841204	1318.855594	16.294247
26.572126	1318.170118	16.299264
26.814597	1311.658265	16.304282
26.809157	1320.712775	16.309299
27.103698	1316.347105	16.314317
27.147442	1314.691571	16.319335
26.788250	1318.932249	16.324352
27.242782	1323.095141	16.329370
26.685284	1317.195922	16.334387
27.061061	1315.932497	16.339405
27.229923	1316.617344	16.344423
27.032216	1324.090685	16.349440
27.182211	1317.308918	16.354458
27.052886	1318.963375	16.359475
27.123286	1305.636117	16.364493
27.294655	1324.218616	16.369511
27.277857	1339.953335	16.374528
27.872720	1339.999761	16.379546
27.135438	1332.746792	16.384563
27.301349	1324.821422	16.389581
27.281573	1336.931392	16.394599
27.353678	1342.716504	16.399616
27.601229	1343.823914	16.404634
27.771596	1347.812743	16.409651
27.768455	1348.278613	16.414669
27.868741	1345.664267	16.419687
27.441339	1337.910942	16.424704
27.446582	1340.032263	16.429722
27.440123	1342.334231	16.434739
27.792064	1344.803710	16.439757
27.739392	1343.743349	16.444775
27.614295	1350.158601	16.449792
27.810340	1336.458441	16.454810
27.765261	1339.527306	16.459827
27.669507	1345.194512	16.464845
27.980116	1341.372752	16.469863
27.545086	1344.059078	16.474880
27.830799	1332.332979	16.479898
27.643113	1341.691986	16.484915
27.914970	1335.324259	16.489933
27.887707	1333.573583	16.494951
27.887916	1345.077198	16.499968
28.059549	1340.767064	16.504986
27.934617	1349.324289	16.510003
28.031385	1334.651905	16.515021
28.084214	1337.577838	16.520039
27.814361	1344.127228	16.525056
28.089705	1340.772447	16.530074
28.214006	1356.650770	16.535091
27.995049	1352.926164	16.540109
28.400217	1366.639897	16.545127
28.274500	1365.699463	16.550144
28.726126	1364.538837	16.555162
28.597194	1358.259377	16.560179
28.603682	1333.606951	16.565197
28.490717	1331.051664	16.570215
28.211539	1341.199295	16.575232
28.538965	1325.139400	16.580250
28.411274	1335.483810	16.585267
28.135833	1330.876749	16.590285
28.574188	1332.595444	16.595303
28.428833	1360.610410	16.600320
28.748207	1356.431345	16.605338
28.706885	1361.783899	16.610355
28.646158	1361.919375	16.615373
28.415839	1354.511762	16.620391
28.268814	1367.030522	16.625408
28.695682	1363.340900	16.630426
28.373427	1370.157583	16.635443
28.490892	1364.966565	16.640461
28.675147	1361.633131	16.645479
28.188723	1364.815283	16.650496
28.480026	1359.935843	16.655514
28.889742	1374.577827	16.660531
28.976580	1387.553749	16.665549
29.063897	1394.380308	16.670567
29.111532	1390.498662	16.675584
29.181506	1391.856844	16.680602
29.262044	1393.480171	16.685619
28.970265	1385.388314	16.690637
29.307823	1381.098183	16.695655
29.094886	1391.384092	16.700672
29.146724	1387.196482	16.705690
29.304159	1384.300679	16.710707
29.182905	1378.031160	16.715725
29.425952	1372.884338	16.720743
29.090642	1375.710073	16.725760
29.394983	1373.252525	16.730778
29.196259	1376.520581	16.735795
29.021629	1381.569432	16.740813
29.637585	1386.357932	16.745831
29.236332	1395.771160	16.750848
29.375937	1378.252308	16.755866
29.339814	1395.667589	16.760883
29.613568	1383.240774	16.765901
29.448915	1379.074771	16.770919
29.332111	1388.557900	16.775936
29.535084	1384.464589	16.780954
29.614188	1389.855511	16.785971
29.505724	1389.255284	16.790989
29.871675	1386.456303	16.796007
29.365458	1393.300248	16.801024
29.607007	1390.424003	16.806042
29.687127	1390.765894	16.811059
29.673226	1393.018714	16.816077
29.942457	1389.358678	16.821095
29.658853	1385.469773	16.826112
29.690524	1381.209131	16.831130
29.687708	1403.038932	16.836147
30.036618	1407.395458	16.841165
30.116975	1414.558167	16.846183
29.970146	1416.887082	16.851200
29.905252	1418.869436	16.856218
30.067667	1420.871304	16.861235
30.157005	1417.617314	16.866253
30.230835	1418.557403	16.871271
30.270498	1415.907598	16.876288
30.359909	1417.647751	16.881306
30.451092	1412.714763	16.886323
29.931837	1412.509538	16.891341
30.478356	1411.795562	16.896359
30.317605	1412.405375	16.901376
30.266270	1416.815055	16.906394
30.360420	1401.643506	16.911411
30.320553	1407.342634	16.916429
30.384998	1414.525293	16.921447
30.217898	1420.925471	16.926464
30.126552	1409.862717	16.931482
30.214122	1415.827755	16.936499
30.109312	1418.942131	16.941517
30.267479	1407.439188	16.946535
30.177881	1417.497872	16.951552
30.149196	1413.593011	16.956570
30.381510	1427.262341	16.961587
30.297182	1439.066569	16.966605
30.695966	1428.959861	16.971623
31.004131	1445.918362	16.976640
30.871246	1436.212259	16.981658
30.870352	1433.114691	16.986675
30.566330	1443.408994	16.991693
31.009358	1436.620083	16.996711
31.033462	1445.101559	17.001728
30.917742	1432.041135	17.006746
31.084761	1439.194652	17.011763
30.978776	1441.535519	17.016781
31.040918	1437.052141	17.021799
30.754019	1445.332685	17.026816
30.756423	1436.598571	17.031834
31.128775	1442.771246	17.036851
30.774423	1438.069925	17.041869
30.877936	1439.184218	17.046887
30.675665	1454.044125	17.051904
31.128228	1452.271221	17.056922
31.279177	1466.862761	17.061939
31.234161	1473.025297	17.066957
31.816451	1464.223879	17.071975
31.514407	1466.732366	17.076992
31.541439	1465.353554	17.082010
31.481194	1458.216956	17.087027
31.308303	1469.560320	17.092045
31.553290	1458.767889	17.097063
31.561322	1455.546024	17.102080
31.665968	1465.472064	17.107098
31.490441	1450.818586	17.112115
31.502012	1465.047582	17.117133
31.527446	1454.123940	17.122151
31.981577	1464.017812	17.127168
31.957296	1460.779242	17.132186
32.216165	1458.786610	17.137203
31.952077	1460.897936	17.142221
31.773213	1431.039133	17.147239
31.702344	1436.489101	17.152256
31.959551	1439.247244	17.157274
32.017653	1451.893371	17.162291
31.662924	1446.643172	17.167309
31.995585	1441.326225	17.172327
31.914910	1453.339083	17.177344
31.698270	1452.478030	17.182362
31.920391	1449.528618	17.187379
31.692533	1454.339473	17.192397
31.673882	1454.853768	17.197415
31.860950	1452.688383	17.202432
31.768698	1450.015693	17.207450
32.020775	1460.386591	17.212467
32.175320	1471.763432	17.217485
32.278159	1480.599975	17.222503
32.349443	1487.152492	17.227520
32.399728	1492.659417	17.232538
32.750221	1487.128120	17.237555
32.400255	1475.138508	17.242573
32.336557	1450.578190	17.247591
32.410204	1459.453988	17.252608
32.260473	1465.379729	17.257626
32.795626	1473.442170	17.262643
32.399720	1485.910238	17.267661
32.987324	1476.083079	17.272679
32.631387	1458.303555	17.277696
32.388302	1450.606905	17.282714
32.676745	1465.705371	17.287731
32.698614	1483.475486	17.292749
32.753058	1478.532803	17.297767
32.636181	1481.741890	17.302784
32.434897	1482.659936	17.307802
32.602869	1483.266012	17.312819
32.789431	1483.943023	17.317837
32.877419	1482.576770	17.322855
32.941528	1480.856247	17.327872
32.732967	1485.462967	17.332890
32.663120	1474.048041	17.337907
32.813071	1487.280509	17.342925
33.010651	1481.474329	17.347943
32.909739	1480.913396	17.352960
32.742901	1486.913812	17.357978
33.006877	1491.543416	17.362995
33.164606	1495.224573	17.368013
33.095794	1507.927738	17.373031
33.362174	1507.957199	17.378048
33.261463	1512.515401	17.383066
33.503045	1498.111803	17.388083
33.403525	1518.414264	17.393101
33.187302	1501.764001	17.398119
33.082668	1510.511044	17.403136
33.265234	1513.095143	17.408154
33.387976	1502.944449	17.413171
33.484538	1505.657704	17.418189
33.597913	1509.378670	17.423207
33.539984	1503.517475	17.428224
33.376085	1517.348410	17.433242
33.734433	1502.789704	17.438259
33.566649	1512.455522	17.443277
33.752280	1527.785773	17.448295
33.995977	1537.935500	17.453312
33.672534	1532.340778	17.458330
34.287773	1524.041685	17.463347
34.081936	1517.179085	17.468365
34.109596	1507.669210	17.473383
34.070700	1501.208300	17.478400
33.874269	1506.256464	17.483418
34.238351	1491.149260	17.488435
34.144911	1507.025537	17.493453
34.068134	1502.599540	17.498471
34.137899	1495.661685	17.503488
34.003677	1514.938722	17.508506
34.215725	1505.559970	17.513523
34.098340	1505.387925	17.518541
34.132142	1509.067521	17.523559
34.173244	1494.187285	17.528576
34.020703	1508.197609	17.533594
34.543762	1523.425645	17.538611
34.586119	1526.905236	17.543629
34.636815	1521.579747	17.548647
34.716597	1504.888241	17.553664
34.303496	1506.710855	17.558682
34.371198	1497.155596	17.563699
34.503119	1494.156326	17.568717
34.178821	1500.543544	17.573735
34.293843	1507.672225	17.578752
34.062641	1524.565045	17.583770
34.580791	1534.946150	17.588787
34.256725	1540.024864	17.593805
34.455479	1535.951499	17.598823
34.606432	1529.961104	17.603840
34.510713	1531.741114	17.608858
34.557890	1537.330644	17.613875
34.317809	1548.529088	17.618893
34.597681	1565.771493	17.623911
34.858928	1563.052175	17.628928
34.594143	1573.872489	17.633946
34.954944	1563.418081	17.638963
34.893208	1551.358537	17.643981
34.920097	1563.597766	17.648999
35.052667	1546.374729	17.654016
34.972130	1561.046535	17.659034
35.137772	1564.706718	17.664051
35.762632	1582.361556	17.669069
35.551735	1568.644591	17.674087
35.659474	1555.541821	17.679104
35.391371	1556.231379	17.684122
35.655700	1548.365407	17.689139
35.627685	1552.060346	17.694157
35.323996	1547.160290	17.699175
35.693351	1545.763872	17.704192
35.393624	1547.145569	17.709210
35.560254	1546.278844	17.714227
35.370467	1550.671486	17.719245
35.431966	1543.815083	17.724263
36.052248	1548.305127	17.729280
35.497444	1549.130436	17.734298
35.498798	1540.073252	17.739315
35.738386	1550.710215	17.744333
35.539883	1551.717163	17.749351
35.742740	1540.790317	17.754368
35.556014	1551.714038	17.759386
35.890736	1562.270139	17.764403
36.038995	1568.338381	17.769421
35.857201	1581.201400	17.774439
36.065183	1575.113386	17.779456
35.788581	1583.893612	17.784474
36.271527	1575.989532	17.789491
36.130621	1572.049836	17.794509
36.072808	1582.283665	17.799527
36.062239	1570.711647	17.804544
35.867959	1580.953856	17.809562
36.462926	1580.249778	17.814579
36.210909	1574.910523	17.819597
36.375111	1582.030915	17.824615
36.250379	1576.078383	17.829632
36.056122	1587.403320	17.834650
36.014777	1578.428750	17.839667
36.443009	1583.549476	17.844685
36.209809	1569.482110	17.849703
36.150909	1580.088311	17.854720
36.473914	1597.549774	17.859738
36.464464	1601.193435	17.864755
36.712878	1598.778554	17.869773
36.669833	1608.174048	17.874791
37.107745	1590.813113	17.879808
37.034518	1601.746653	17.884826
36.783653	1601.042802	17.889843
36.982753	1593.577692	17.894861
36.674847	1596.977797	17.899879
36.829082	1591.920569	17.904896
36.754952	1595.288144	17.909914
36.929186	1594.070797	17.914931
37.168357	1590.984110	17.919949
37.138929	1591.872385	17.924967
37.047150	1588.478823	17.929984
36.957184	1599.248614	17.935002
36.784186	1591.762329	17.940019
37.074716	1592.859900	17.945037
36.834962	1585.692088	17.950055
37.113037	1587.473515	17.955072
37.043552	1589.547188	17.960090
37.254775	1592.112984	17.965107
37.426007	1597.995773	17.970125
37.346316	1603.567124	17.975143
37.830469	1605.647722	17.980160
37.583540	1599.775996	17.985178
37.421723	1592.898017	17.990195
37.826729	1592.531785	17.995213
37.382779	1592.583170	18.000231
37.332753	1589.104372	18.005248
37.697663	1600.511498	18.010266
37.743563	1614.578485	18.015283
37.995883	1620.286683	18.020301
37.966543	1615.778219	18.025319
37.918769	1609.683839	18.030336
37.706407	1595.789360	18.035354
37.471691	1604.119035	18.040371
38.052687	1610.391534	18.045389
37.963872	1627.713042	18.050407
38.230711	1624.985114	18.055424
38.374167	1619.508256	18.060442
38.306204	1613.213302	18.065459
37.891806	1596.566554	18.070477
38.093813	1619.477234	18.075495
38.160702	1621.207748	18.080512
38.156812	1620.573501	18.085530
38.152994	1618.874816	18.090547
38.079510	1618.551637	18.095565
37.960157	1620.400121	18.100583
38.331601	1608.987554	18.105600
38.176119	1621.066440	18.110618
38.124558	1625.176256	18.115635
38.562670	1611.666135	18.120653
38.233734	1627.941444	18.125671
38.438707	1625.460126	18.130688
38.810664	1637.519966	18.135706
38.800217	1636.292588	18.140723
38.529286	1630.570664	18.145741
38.350573	1634.133853	18.150759
38.675381	1635.787696	18.155776
38.683643	1648.650265	18.160794
38.565315	1647.988675	18.165811
38.744823	1642.611743	18.170829
38.789462	1650.453211	18.175847
38.987086	1642.834404	18.180864
39.074456	1642.887543	18.185882
38.732633	1637.525907	18.190899
39.199660	1630.142472	18.195917
38.925266	1638.919806	18.200935
39.059105	1634.934101	18.205952
39.162769	1641.568724	18.210970
39.064811	1641.153538	18.215987
39.216178	1652.250957	18.221005
39.091422	1653.032564	18.226023
39.334715	1665.880124	18.231040
39.474730	1669.129464	18.236058
39.333357	1669.561304	18.241075
39.971168	1676.071063	18.246093
39.829572	1662.163058	18.251111
39.839484	1648.116460	18.256128
39.638075	1637.725581	18.261146
39.333504	1635.107430	18.266163
39.562753	1622.170523	18.271181
39.468514	1638.616481	18.276199
39.440950	1645.614281	18.281216
39.949501	1648.228382	18.286234
39.808965	1663.983486	18.291251
39.936563	1662.275283	18.296269
39.887552	1660.129199	18.301287
40.014050	1659.131126	18.306304
39.848594	1657.601845	18.311322
39.890731	1670.511387	18.316339
40.165845	1655.727543	18.321357
40.136462	1655.750179	18.326375
40.000325	1653.831655	18.331392
40.421190	1652.739077	18.336410
40.107629	1658.476047	18.341427
40.192119	1657.629385	18.346445
39.946604	1668.754808	18.351463
40.186544	1659.244008	18.356480
40.434551	1661.921438	18.361498
40.169436	1665.091091	18.366515
40.293101	1653.708218	18.371533
40.263808	1658.858913	18.376551
40.263277	1655.528987	18.381568
40.241250	1664.507710	18.386586
40.093796	1667.451451	18.391603
40.463364	1675.319344	18.396621
40.534208	1679.673874	18.401639
40.811711	1683.129996	18.406656
40.931808	1676.833265	18.411674
40.568330	1684.174548	18.416691
40.866914	1676.270375	18.421709
40.687184	1675.148321	18.426727
40.868447	1678.124345	18.431744
41.026568	1673.883863	18.436762
40.874849	1684.725525	18.441779
40.842292	1681.897475	18.446797
40.736444	1679.555493	18.451815
40.842440	1694.146017	18.456832
41.162552	1691.435846	18.461850
40.974397	1723.340136	18.466867
41.106921	1705.235346	18.471885
41.297561	1704.055629	18.476903
41.460862	1703.774213	18.481920
41.168353	1695.798636	18.486938
40.977870	1707.460396	18.491955
41.274030	1697.964491	18.496973
41.332114	1701.549383	18.501991
41.708386	1702.933937	18.507008
41.577835	1701.006020	18.512026
41.275906	1698.368723	18.517043
41.617011	1697.995335	18.522061
41.820784	1721.747894	18.527079
41.725933	1730.343661	18.532096
42.070307	1724.219075	18.537114
41.910755	1720.921318	18.542131
41.915937	1706.862458	18.547149
41.918174	1714.654083	18.552167
42.203171	1710.747500	18.557184
41.918225	1699.927920	18.562202
41.880165	1711.820565	18.567219
42.140965	1710.593234	18.572237
42.095903	1709.162148	18.577255
42.123166	1720.996177	18.582272
42.187466	1728.086301	18.587290
41.852252	1730.729627	18.592307
42.023518	1725.400283	18.597325
41.916401	1721.948997	18.602343
41.896370	1720.883806	18.607360
42.553037	1725.322621	18.612378
42.298969	1722.280019	18.617395
42.130591	1720.868130	18.622413
42.415278	1733.225306	18.627431
42.491888	1717.037771	18.632448
42.547566	1731.129820	18.637466
42.888938	1752.690274	18.642483
42.642114	1753.189536	18.647501
43.155128	1744.109877	18.652519
42.922594	1736.358590	18.657536
43.161363	1727.831086	18.662554
42.920235	1722.412037	18.667571
42.862526	1714.935770	18.672589
43.040012	1716.137847	18.677607
42.640361	1727.704480	18.682624
42.841393	1718.917896	18.687642
42.677113	1746.076562	18.692659
43.055616	1743.446879	18.697677
43.088882	1746.025576	18.702695
42.982490	1761.416520	18.707712
43.201596	1741.679272	18.712730
43.138031	1749.615827	18.717747
43.234209	1745.580812	18.722765
43.338907	1752.727256	18.727783
43.211053	1753.730415	18.732800
43.333258	1752.539762	18.737818
43.209567	1756.807775	18.742835
43.457616	1756.555459	18.747853
43.497445	1766.901803	18.752871
43.318703	1779.274975	18.757888
43.754667	1774.622061	18.762906
43.614863	1771.236788	18.767923
43.816074	1779.091616	18.772941
44.023031	1769.305524	18.777959
44.078683	1769.877031	18.782976
43.865005	1780.937832	18.787994
44.056682	1771.331408	18.793011
43.902783	1775.100149	18.798029
44.178684	1770.461286	18.803047
43.784014	1774.317446	18.808064
43.734929	1772.441798	18.813082
43.697569	1771.306642	18.818099
44.053432	1779.051869	18.823117
44.432982	1772.446902	18.828135
43.998026	1782.617810	18.833152
44.591407	1794.409518	18.838170
44.469799	1809.879198	18.843187
44.424261	1803.426147	18.848205
44.844485	1796.301125	18.853223
44.314856	1786.061813	18.858240
44.912428	1775.391386	18.863258
44.358473	1781.587761	18.868275
44.529995	1782.574910	18.873293
44.693140	1798.170926	18.878311
44.249318	1798.001843	18.883328
44.609518	1792.317081	18.888346
44.524807	1802.617502	18.893363
44.758206	1796.963534	18.898381
44.947648	1793.776180	18.903399
44.431101	1793.070756	18.908416
44.656746	1798.208499	18.913434
44.931991	1813.551192	18.918451
45.212082	1818.203033	18.923469
45.532138	1828.830828	18.928487
45.295837	1815.136933	18.933504
45.291859	1803.468780	18.938522
44.856052	1794.982643	18.943539
44.752203	1811.624444	18.948557
45.327512	1819.691062	18.953575
45.432073	1821.941099	18.958592
45.251641	1827.620112	18.963610
45.521611	1830.055389	18.968627
45.611779	1830.820187	18.973645
45.864227	1819.440907	18.978663
45.645072	1821.726920	18.983680
45.510321	1824.084408	18.988698
45.879241	1822.900612	18.993715
45.777903	1824.090316	18.998733
45.879435	1818.965157	19.003751
45.848046	1824.418580	19.008768
45.926222	1821.495443	19.013786
45.913141	1822.661902	19.018803
45.956215	1821.071180	19.023821
46.113803	1819.719772	19.028839
45.820778	1821.609576	19.033856
46.007487	1823.041409	19.038874
46.040014	1819.401887	19.043891
46.004273	1818.526862	19.048909
46.302994	1818.725172	19.053927
46.008248	1832.953558	19.058944
46.148723	1839.662489	19.063962
46.447960	1849.289723	19.068979
46.292491	1855.276593	19.073997
46.304020	1854.733675	19.079015
46.032150	1860.787021	19.084032
46.428123	1860.257139	19.089050
46.792875	1847.522232	19.094067
46.302972	1850.474374	19.099085
46.728536	1844.997860	19.104103
46.799230	1846.710647	19.109120
46.756825	1844.921278	19.114138
46.731201	1852.488863	19.119155
46.658140	1864.920813	19.124173
47.106093	1863.812919	19.129191
47.040514	1868.419154	19.134208
46.939573	1874.910150	19.139226
47.323833	1878.568530	19.144243
47.344090	1879.002009	19.149261
47.391399	1870.835162	19.154279
47.592351	1872.068999	19.159296
47.593080	1857.896380	19.164314
47.450759	1846.831303	19.169331
47.064939	1846.201703	19.174349
47.621065	1841.063415	19.179367
47.157045	1844.364584	19.184384
47.398746	1853.100253	19.189402
47.480925	1859.110838	19.194419
47.257822	1865.938909	19.199437
47.269654	1860.470727	19.204455
47.637692	1872.275918	19.209472
47.745942	1863.993504	19.214490
47.747083	1866.107506	19.219507
47.170711	1867.644972	19.224525
47.648608	1862.652660	19.229543
47.903361	1891.661406	19.234560
47.983725	1886.700137	19.239578
48.153278	1892.591387	19.244595
47.864254	1888.732772	19.249613
48.197560	1894.290305	19.254631
47.831141	1894.577864	19.259648
47.785315	1895.579286	19.264666
48.300777	1881.376698	19.269683
48.193590	1894.459315	19.274701
48.131852	1886.223875	19.279719
48.349401	1879.861750	19.284736
48.401041	1886.672379	19.289754
48.372734	1879.478542	19.294771
48.556030	1885.128569	19.299789
48.769298	1891.317284	19.304807
48.451400	1886.373212	19.309824
48.530982	1902.061480	19.314842
48.898360	1904.341712	19.319859
48.640931	1905.898909	19.324877
48.900410	1905.730717	19.329895
49.059880	1902.649069	19.334912
48.985535	1910.961855	19.339930
49.418262	1908.522965	19.344947
48.986730	1911.093270	19.349965
49.298537	1908.225397	19.354983
49.311066	1904.572232	19.360000
49.160197	1904.701942	19.365018
49.530670	1898.145267	19.370035
49.254676	1891.612362	19.375053
49.201442	1895.700876	19.380071
49.274684	1900.574305	19.385088
48.900438	1908.567989	19.390106
49.000014	1899.229433	19.395123
48.940666	1897.423174	19.400141
49.109973	1904.327346	19.405159
49.207548	1926.579833	19.410176
49.758814	1933.283316	19.415194
49.630080	1921.891369	19.420211
49.957594	1929.849012	19.425229
50.154233	1928.049065	19.430247
50.314276	1928.888137	19.435264
49.927082	1928.256792	19.440282
50.463364	1924.321229	19.445299
50.115663	1926.234449	19.450317
50.306432	1922.480574	19.455335
50.276894	1907.098088	19.460352
49.920968	1903.606389	19.465370
50.236841	1902.396712	19.470387
49.852419	1926.923482	19.475405
50.145520	1924.797984	19.480423
50.330656	1917.293101	19.485440
50.189191	1926.147045	19.490458
50.684754	1914.822589	19.495475
50.162685	1924.213586	19.500493
50.330466	1926.092601	19.505511
50.365421	1928.189017	19.510528
50.130693	1925.182937	19.515546
51.054490	1935.929322	19.520563
50.805358	1946.768763	19.525581
51.074373	1941.729457	19.530599
50.560867	1950.590374	19.535616
50.760006	1948.035174	19.540634
50.690215	1946.735304	19.545651
50.690416	1939.583966	19.550669
51.005595	1942.619991	19.555687
51.399823	1946.346812	19.560704
51.085527	1947.264270	19.565722
51.259146	1945.882843	19.570739
51.141355	1944.873157	19.575757
51.065400	1942.062072	19.580775
51.238701	1947.225836	19.585792
51.335185	1962.198657	19.590810
51.619444	1968.527623	19.595827
51.681392	1979.187153	19.600845
51.945262	1975.244433	19.605863
51.795741	1953.702481	19.610880
51.625966	1948.649078	19.615898
51.626548	1940.441692	19.620915
51.667750	1951.262881	19.625933
51.586409	1960.600949	19.630951
51.969074	1964.138958	19.635968
51.900594	1978.880422	19.640986
51.934979	1966.684800	19.646003
52.010506	1968.736528	19.651021
51.975455	1968.886465	19.656039
52.304758	1966.321955	19.661056
52.214076	1960.774232	19.666074
52.446025	1964.512718	19.671091
52.529997	1966.055627	19.676109
52.326691	1972.394897	19.681127
52.487031	1958.746930	19.686144
52.408981	1967.086144	19.691162
52.414418	1963.489446	19.696179
52.240533	1968.969813	19.701197
52.527547	1966.500471	19.706215
52.521534	1967.646878	19.711232
52.364534	1965.732746	19.716250
52.513259	1967.608223	19.721267
52.358650	1973.400333	19.726285
52.261071	1982.770426	19.731303
52.539443	1985.735384	19.736320
52.793559	1997.531351	19.741338
52.788531	1998.143205	19.746355
52.429511	1997.415282	19.751373
52.612175	2015.997145	19.756391
53.060355	2022.068166	19.761408
52.857479	2033.180506	19.766426
53.197484	2022.700095	19.771443
53.121694	2025.062632	19.776461
52.343147	2027.677113	19.781479
52.989402	2034.229131	19.786496
53.574962	2056.322238	19.791514
53.761117	2043.290339	19.796531
53.761976	2047.906513	19.801549
53.899219	2036.226263	19.806567
54.011981	2033.557383	19.811584
53.972273	2044.753387	19.816602
54.736276	2038.047970	19.821619
54.504654	2047.238896	19.826637
54.394541	2024.541437	19.831655
54.444022	2013.564217	19.836672
54.022908	2017.723987	19.841690
54.087140	2007.214165	19.846707
54.342693	2010.612381	19.851725
54.296740	1991.222519	19.856743
54.232071	1999.390265	19.861760
54.051607	2013.559386	19.866778
54.240727	2012.150984	19.871795
54.287362	2012.985380	19.876813
53.879715	2020.194962	19.881831
54.328378	2026.496195	19.886848
54.224443	2027.943796	19.891866
54.285108	2030.019050	19.896883
54.097591	2042.588744	19.901901
54.225696	2053.848943	19.906919
54.701474	2062.468106	19.911936
54.723658	2064.290104	19.916954
54.834118	2066.866334	19.921971
54.778199	2074.860842	19.926989
54.722821	2066.398687	19.932007
54.675622	2066.285501	19.937024
54.664086	2071.014348	19.942042
54.819191	2078.702755	19.947059
55.301443	2096.821275	19.952077
55.641530	2084.627793	19.957095
55.788558	2084.451019	19.962112
55.703059	2094.661617	19.967130
55.634999	2074.939510	19.972147
55.665766	2061.683496	19.977165
55.166680	2060.801765	19.982183
55.564978	2058.854514	19.987200
55.658003	2082.262190	19.992218
55.922211	2077.339174	19.997235
55.928122	2083.394926	20.002253
56.140570	2087.968077	20.007271
55.924979	2069.835354	20.012288
55.464424	2069.767643	20.017306
55.705760	2072.532264	20.022323
55.710629	2078.093946	20.027341
55.717592	2079.523817	20.032359
56.090152	2073.016916	20.037376
56.149219	2083.417965	20.042394
56.139483	2073.291543	20.047411
56.244466	2082.890795	20.052429
56.261615	2095.214135	20.057447
56.640968	2093.096800	20.062464
56.612606	2116.617687	20.067482
56.694008	2110.090190	20.072499
56.665515	2107.163369	20.077517
56.540464	2114.115884	20.082535
57.131097	2093.439911	20.087552
56.531397	2109.693154	20.092570
56.581086	2100.954589	20.097587
56.909986	2099.333337	20.102605
56.547311	2108.597918	20.107623
56.890799	2109.604699	20.112640
56.665539	2104.525574	20.117658
56.670264	2105.837325	20.122675
57.122103	2117.548551	20.127693
57.119105	2133.433950	20.132711
57.052219	2123.738748	20.137728
56.842467	2137.764412	20.142746
57.285455	2133.209040	20.147763
57.616319	2129.891368	20.152781
57.262067	2140.272379	20.157799
57.761243	2132.759391	20.162816
57.564791	2134.289803	20.167834
57.664185	2137.519383	20.172851
57.640559	2136.632890	20.177869
57.868805	2162.745632	20.182887
58.103416	2152.888987	20.187904
58.176526	2167.063782	20.192922
58.426110	2140.743869	20.197939
58.065297	2125.004334	20.202957
58.044337	2124.705137	20.207975
58.269865	2124.462246	20.212992
58.295629	2129.797092	20.218010
58.212529	2131.743572	20.223027
58.583176	2148.726183	20.228045
58.143354	2156.324966	20.233063
58.610432	2143.038510	20.238080
58.352265	2155.583951	20.243098
58.118816	2150.623475	20.248115
58.437371	2150.639594	20.253133
58.422363	2147.385175	20.258151
58.852994	2145.285342	20.263168
58.853431	2155.646921	20.268186
58.705555	2154.260143	20.273203
58.725630	2147.470940	20.278221
58.612183	2149.286625	20.283239
59.073030	2160.600370	20.288256
59.070133	2182.555097	20.293274
59.607782	2177.708703	20.298291
59.437593	2158.430883	20.303309
59.233448	2150.234581	20.308327
59.012251	2150.642816	20.313344
58.931573	2157.853937	20.318362
58.889490	2166.103267	20.323379
59.311639	2169.198622	20.328397
59.102754	2169.619192	20.333415
59.086816	2179.102869	20.338432
59.580592	2190.947955	20.343450
59.584296	2209.442707	20.348467
59.725422	2207.204109	20.353485
59.774408	2204.798077	20.358503
59.932159	2194.762589	20.363520
59.802245	2211.632139	20.368538
59.787116	2205.370136	20.373555
60.101031	2209.229574	20.378573
59.812106	2209.976531	20.383591
60.291740	2204.638187	20.388608
59.811516	2194.942549	20.393626
59.986462	2205.924082	20.398643
60.265659	2220.582735	20.403661
60.172297	2217.972293	20.408679
60.389697	2227.814057	20.413696
60.521189	2232.354963	20.418714
60.513021	2234.851818	20.423731
60.660104	2225.184968	20.428749
60.895730	2224.006635	20.433767
60.808676	2226.199624	20.438784
60.973104	2221.524920	20.443802
60.790175	2223.781975	20.448819
60.879464	2223.178168	20.453837
60.775687	2241.293511	20.458855
61.199799	2246.048838	20.463872
61.313188	2248.819084	20.468890
61.036586	2262.325248	20.473907
61.628351	2245.700487	20.478925
61.623619	2255.596101	20.483943
61.369717	2242.047043	20.488960
61.941851	2236.658958	20.493978
61.773641	2249.801364	20.498995
61.829183	2246.558099	20.504013
62.012584	2243.455698	20.509031
62.119068	2226.373404	20.514048
61.769797	2214.355344	20.519066
61.491983	2215.654941	20.524083
61.964996	2213.973645	20.529101
61.870274	2236.079043	20.534119
61.848354	2240.424457	20.539136
61.994860	2238.813057	20.544154
61.729549	2238.560536	20.549171
62.078515	2230.644212	20.554189
62.276193	2237.662929	20.559207
62.123719	2242.759969	20.564224
62.253595	2240.017366	20.569242
62.211093	2257.837591	20.574259
62.602116	2265.980369	20.579277
62.576819	2267.464008	20.584295
62.703876	2267.397610	20.589312
62.880925	2279.026820	20.594330
62.473515	2277.070572	20.599347
62.841488	2267.483325	20.604365
62.772563	2272.841543	20.609383
62.709212	2274.700534	20.614400
62.335644	2267.421849	20.619418
62.640670	2281.885562	20.624435
62.974533	2293.344985	20.629453
62.920231	2296.490951	20.634471
63.031830	2296.231455	20.639488
63.175382	2290.959838	20.644506
62.950346	2298.294083	20.649523
63.304879	2295.987336	20.654541
63.016968	2298.222384	20.659559
63.194276	2312.650543	20.664576
63.865358	2313.241424	20.669594
63.357084	2319.064155	20.674611
63.857835	2322.593561	20.679629
63.794355	2318.424755	20.684647
63.714430	2318.588605	20.689664
64.110017	2310.885581	20.694682
63.482524	2324.535995	20.699699
63.676154	2322.053489	20.704717
63.796246	2333.338639	20.709735
64.259478	2338.348531	20.714752
64.528192	2349.435724	20.719770
64.529179	2356.250207	20.724787
64.699476	2345.562209	20.729805
64.529533	2338.350227	20.734823
64.677899	2345.093112	20.739840
65.059233	2339.522168	20.744858
64.975571	2346.464995	20.749875
64.981417	2329.483660	20.754893
65.141509	2327.873745	20.759911
64.863196	2316.519412	20.764928
64.855721	2310.147253	20.769946
65.016889	2335.309449	20.774963
64.993553	2329.992175	20.779981
65.028447	2341.919309	20.784999
64.858412	2337.080173	20.790016
65.598480	2341.501059	20.795034
64.919105	2342.482607	20.800051
65.129113	2334.972822	20.805069
65.180836	2338.953172	20.810087
65.492981	2340.881015	20.815104
65.549149	2339.882710	20.820122
65.449675	2348.602409	20.825139
65.559763	2360.367932	20.830157
65.741583	2369.080920	20.835175
66.025639	2365.860886	20.840192
66.023709	2360.501682	20.845210
65.768249	2370.205947	20.850227
65.915990	2364.015776	20.855245
65.912761	2371.793480	20.860263
65.867861	2370.427458	20.865280
65.944860	2371.853657	20.870298
65.956663	2383.662799	20.875315
65.863527	2393.470952	20.880333
66.224345	2395.214199	20.885351
66.005945	2393.284964	20.890368
66.336145	2394.028234	20.895386
66.296978	2399.294578	20.900403
66.722464	2400.550997	20.905421
67.060419	2413.003453	20.910439
67.031077	2413.115839	20.915456
67.422586	2398.518335	20.920474
67.216523	2389.542954	20.925491
67.420774	2387.090767	20.930509
67.172295	2374.405978	20.935527
67.151576	2375.814863	20.940544
67.376750	2368.307083	20.945562
66.949021	2379.887697	20.950579
67.534842	2384.904511	20.955597
67.339552	2397.103761	20.960615
67.723538	2391.194200	20.965632
68.038248	2391.797128	20.970650
67.607270	2386.118688	20.975667
67.813148	2384.392550	20.980685
67.753030	2378.317818	20.985703
67.811813	2381.654940	20.990720
67.793003	2374.586063	20.995738
67.992688	2390.541573	21.000755
67.624317	2386.699879	21.005773
67.737000	2396.132910	21.010791
67.574426	2395.462063	21.015808
67.876073	2391.602162	21.020826
67.880266	2406.325726	21.025843
68.137685	2418.737956	21.030861
68.331875	2413.339436	21.035879
68.401581	2425.338828	21.040896
68.649756	2422.396738	21.045914
68.556142	2423.193510	21.050931
68.499286	2425.739185	21.055949
68.800016	2425.026420	21.060967
68.612395	2430.392300	21.065984
68.693216	2424.432832	21.071002
68.791264	2427.956964	21.076019
68.755848	2443.175848	21.081037
68.703305	2441.579802	21.086055
68.874828	2447.549674	21.091072
69.221358	2440.313908	21.096090
69.438570	2438.491411	21.101107
69.281216	2453.366311	21.106125
69.147652	2444.162596	21.111143
69.140713	2458.041069	21.116160
69.703552	2468.529590	21.121178
69.927602	2464.166786	21.126195
69.774030	2476.660756	21.131213
69.740583	2472.620400	21.136231
69.880207	2476.658301	21.141248
69.842915	2465.358511	21.146266
69.797984	2462.921112	21.151283
69.543026	2461.165220	21.156301
70.004095	2458.147395	21.161319
70.213066	2485.088214	21.166336
70.349906	2488.399273	21.171354
70.662997	2501.036210	21.176371
70.953465	2482.529044	21.181389
71.026564	2469.441852	21.186407
70.838008	2462.976531	21.191424
71.027439	2455.218926	21.196442
70.905098	2451.827073	21.201459
70.818151	2450.657544	21.206477
70.921513	2451.717414	21.211495
70.830050	2450.688187	21.216512
70.681959	2450.249178	21.221530
71.081987	2470.787052	21.226547
71.470854	2478.717127	21.231565
71.216402	2486.085256	21.236583
71.331367	2489.349933	21.241600
71.400927	2480.350409	21.246618
71.413736	2480.901859	21.251635
71.480659	2488.184405	21.256653
71.227677	2483.909871	21.261671
71.474798	2478.900779	21.266688
71.136810	2482.150153	21.271706
71.333487	2490.222614	21.276723
71.707266	2508.248531	21.281741
71.734910	2512.493712	21.286759
71.705767	2524.589038	21.291776
71.881806	2513.826949	21.296794
71.588144	2508.796982	21.301811
71.757956	2531.244689	21.306829
72.462664	2533.278541	21.311847
72.324531	2529.078907	21.316864
72.233143	2532.562521	21.321882
72.882745	2527.136931	21.326899
72.614686	2538.682028	21.331917
72.901435	2532.994569	21.336935
72.663287	2543.421225	21.341952
72.550819	2527.781764	21.346970
72.661981	2539.523430	21.351987
72.566714	2545.213630	21.357005
73.092874	2538.210322	21.362023
72.850250	2545.045263	21.367040
72.676571	2539.492937	21.372058
72.761508	2560.650476	21.377075
72.930829	2573.313987	21.382093
73.172339	2574.735655	21.387111
72.847691	2581.224153	21.392128
73.280899	2570.009124	21.397146
73.576645	2590.423257	21.402163
73.373955	2594.996464	21.407181
73.666615	2600.938898	21.412199
73.736647	2604.947391	21.417216
73.780536	2601.813450	21.422234
74.057228	2602.270318	21.427251
73.934387	2594.526453	21.432269
74.073290	2612.748577	21.437287
73.712123	2608.344257	21.442304
74.027450	2606.751967	21.447322
74.283211	2617.062413	21.452339
74.068220	2627.665601	21.457357
74.409004	2622.449858	21.462375
74.543381	2622.316702	21.467392
74.394936	2622.727689	21.472410
74.326661	2621.349957	21.477427
74.455518	2619.527670	21.482445
74.735508	2635.414654	21.487463
74.855073	2644.001283	21.492480
75.099396	2653.133012	21.497498
75.112320	2651.915076	21.502515
75.200662	2653.077239	21.507533
75.285962	2650.389171	21.512551
75.567144	2644.366787	21.517568
75.635934	2651.215469	21.522586
75.666914	2649.928215	21.527603
75.704588	2642.008402	21.532621
75.756514	2646.324996	21.537639
75.452153	2651.111070	21.542656
75.165265	2644.743806	21.547674
75.392466	2637.371575	21.552691
75.530521	2664.380132	21.557709
75.915298	2666.554069	21.562727
76.082776	2665.418854	21.567744
76.181346	2676.935160	21.572762
76.342486	2670.084034	21.577779
75.830544	2687.470942	21.582797
75.900563	2670.437488	21.587815
76.256306	2671.285994	21.592832
76.316756	2687.580350	21.597850
76.866313	2690.623068	21.602867
76.627422	2693.071710	21.607885
77.052833	2695.756621	21.612903
76.755536	2698.134605	21.617920
77.008596	2698.661126	21.622938
77.315538	2695.421103	21.627955
77.091392	2700.739965	21.632973
77.389135	2689.416535	21.637991
77.401664	2691.510659	21.643008
77.217314	2688.873835	21.648026
77.311488	2687.103135	21.653043
77.251618	2691.179964	21.658061
77.459221	2690.049533	21.663079
77.516728	2690.058795	21.668096
77.493352	2690.544387	21.673114
77.413506	2684.035420	21.678131
77.301602	2695.941222	21.683149
77.424209	2698.962767	21.688167
77.573097	2715.305920	21.693184
77.590948	2723.218104	21.698202
77.564304	2728.655512	21.703219
77.843384	2736.833966	21.708237
77.952969	2732.619128	21.713255
78.149226	2757.616184	21.718272
78.101840	2753.309176	21.723290
78.384890	2755.473166	21.728307
78.293018	2754.420169	21.733325
78.420158	2749.618601	21.738343
78.832684	2745.982796	21.743360
78.556516	2774.108159	21.748378
79.055006	2762.940075	21.753395
79.135416	2770.376225	21.758413
79.265902	2776.782902	21.763431
79.658308	2768.688468	21.768448
79.227701	2767.508778	21.773466
79.527436	2763.386125	21.778483
79.469518	2757.003417	21.783501
79.645598	2766.457102	21.788519
79.861043	2763.182975	21.793536
79.790223	2756.879954	21.798554
79.888519	2763.867109	21.803571
79.839734	2761.998770	21.808589
79.820990	2772.060997	21.813607
79.840025	2763.181068	21.818624
79.811436	2761.190502	21.823642
80.100498	2759.515928	21.828659
80.008306	2764.851194	21.833677
79.900805	2756.836618	21.838695
79.994852	2758.932240	21.843712
80.066016	2771.123578	21.848730
80.262974	2771.605438	21.853747
80.407767	2775.005987	21.858765
80.684231	2778.378086	21.863783
80.619690	2773.731406	21.868800
80.647292	2781.074325	21.873818
80.414029	2778.976641	21.878835
80.527151	2792.862935	21.883853
80.782415	2799.473400	21.888871
81.050462	2803.631891	21.893888
80.929064	2806.778419	21.898906
81.345367	2803.014031	21.903923
81.383163	2807.039714	21.908941
81.317080	2805.208085	21.913959
81.601062	2815.065207	21.918976
81.439310	2827.969451	21.923994
81.648125	2836.181222	21.929011
81.593336	2844.045632	21.934029
81.562673	2833.229491	21.939047
81.861205	2834.127616	21.944064
81.455540	2836.638482	21.949082
82.272791	2824.121687	21.954099
82.037908	2845.380494	21.959117
82.121282	2853.914562	21.964135
82.536812	2857.070401	21.969152
82.092980	2872.886500	21.974170
82.519132	2869.045277	21.979187
82.292708	2870.145105	21.984205
82.362262	2866.106522	21.989223
82.575142	2870.713495	21.994240
82.338819	2865.269625	21.999258
82.829690	2870.927062	22.004275
82.709671	2880.122281	22.009293
82.721310	2887.075388	22.014311
83.012363	2884.944983	22.019328
82.944466	2889.691661	22.024346
83.434530	2886.679200	22.029363
83.113453	2895.708449	22.034381
83.331510	2903.962822	22.039399
83.938278	2903.018372	22.044416
83.808651	2910.651888	22.049434
84.201522	2903.144681	22.054451
83.925975	2893.933453	22.059469
84.141413	2892.911944	22.064487
84.058481	2878.308141	22.069504
84.097611	2893.079935	22.074522
84.167099	2908.771092	22.079539
83.933225	2916.048626	22.084557
84.187186	2903.097709	22.089575
84.386467	2903.098504	22.094592
83.975160	2907.607854	22.099610
84.377984	2902.574079	22.104627
84.259476	2924.477904	22.109645
84.119258	2937.626701	22.114663
84.717913	2926.158497	22.119680
84.704524	2935.925865	22.124698
84.860506	2921.262464	22.129715
84.596397	2945.465860	22.134733
84.662309	2965.618483	22.139751
85.174164	2969.812712	22.144768
85.122801	2962.752095	22.149786
85.152126	2969.559017	22.154803
85.338090	2977.930144	22.159821
85.273123	2987.490722	22.164839
85.934688	2993.218026	22.169856
86.314123	2990.116744	22.174874
86.390909	2988.846893	22.179891
86.173351	2986.879256	22.184909
86.144028	2982.010561	22.189927
86.664621	2976.962026	22.194944
86.501714	2964.480319	22.199962
86.444950	2954.431363	22.204979
86.085800	2960.814307	22.209997
86.231651	2968.684207	22.215015
86.607271	2973.757998	22.220032
86.510865	2989.142412	22.225050
86.533777	2976.942574	22.230067
86.585707	2972.161633	22.235085
86.553457	2975.876508	22.240103
86.556513	2980.035924	22.245120
86.411743	3015.558190	22.250138
86.855913	3014.114247	22.255155
86.634375	3009.718627	22.260173
87.024787	3025.096252	22.265191
87.169795	3028.819249	22.270208
87.241142	3037.386900	22.275226
87.348694	3038.336281	22.280243
87.475657	3037.323477	22.285261
87.319161	3050.075862	22.290279
87.712426	3054.431438	22.295296
87.858215	3070.057003	22.300314
88.108831	3064.894789	22.305331
88.416151	3061.749901	22.310349
88.680526	3066.542511	22.315367
88.608262	3060.188426	22.320384
88.685892	3060.195545	22.325402
88.897536	3047.058200	22.330419
88.813016	3057.835784	22.335437
88.541673	3054.371967	22.340455
88.809208	3054.057953	22.345472
88.734079	3054.118266	22.350490
88.871437	3054.592662	22.355507
89.029499	3058.167452	22.360525
88.859336	3053.963322	22.365543
88.950968	3044.084660	22.370560
89.076398	3055.930262	22.375578
88.972025	3048.113829	22.380595
89.265328	3062.857958	22.385613
89.036441	3070.070569	22.390631
89.201601	3077.892454	22.395648
89.178083	3082.419661	22.400666
89.021738	3081.217064	22.405683
89.318137	3105.155261	22.410701
89.379540	3121.609753	22.415719
89.915159	3113.278491	22.420736
89.876072	3119.531449	22.425754
90.190438	3129.814051	22.430771
90.500335	3134.261376	22.435789
90.337027	3130.678905	22.440807
90.765219	3128.884455	22.445824
90.852083	3132.296624	22.450842
90.917402	3131.648713	22.455859
91.170388	3120.508344	22.460877
91.038924	3129.800874	22.465895
91.153411	3129.023190	22.470912
90.916326	3125.672589	22.475930
91.148240	3121.563411	22.480947
91.119652	3132.177479	22.485965
91.212338	3127.725964	22.490983
91.449892	3126.722833	22.496000
91.416728	3125.119182	22.501018
91.159478	3128.861038	22.506035
91.682312	3130.652794	22.511053
91.746902	3152.494403	22.516071
91.953363	3162.216530	22.521088
92.058202	3158.503919	22.526106
92.294353	3153.404302	22.531123
92.362578	3141.012601	22.536141
92.050995	3147.918451	22.541159
92.108473	3148.937922	22.546176
92.416682	3148.287275	22.551194
92.373249	3157.932586	22.556211
92.670947	3158.844255	22.561229
92.347506	3174.940363	22.566247
92.344180	3172.810927	22.571264
92.698296	3172.025926	22.576282
92.848422	3185.715519	22.581299
92.715186	3172.475614	22.586317
92.454147	3190.892456	22.591335
92.633518	3195.700727	22.596352
93.132421	3195.616187	22.601370
93.222864	3216.588287	22.606387
93.798426	3219.730750	22.611405
93.601045	3227.554746	22.616423
93.805985	3221.072114	22.621440
93.790190	3227.622832	22.626458
93.692325	3225.262562	22.631475
93.975955	3210.787237	22.636493
93.907429	3229.087670	22.641511
94.142187	3223.389064	22.646528
94.409771	3223.812419	22.651546
94.192236	3249.723506	22.656563
94.480735	3245.905725	22.661581
94.474848	3246.380569	22.666599
94.875224	3239.507771	22.671616
95.012719	3246.006002	22.676634
95.035115	3245.281324	22.681651
95.529853	3248.964300	22.686669
95.002333	3245.024674	22.691687
95.301227	3239.983163	22.696704
95.309590	3241.049731	22.701722
95.086439	3251.528712	22.706739
95.572807	3238.050543	22.711757
95.110367	3246.581715	22.716775
95.114613	3241.757391	22.721792
95.075747	3242.248314	22.726810
95.021870	3266.599356	22.731827
95.907002	3262.725501	22.736845
95.464780	3271.262794	22.741863
95.572057	3275.029092	22.746880
95.682072	3289.649792	22.751898
95.868353	3308.889292	22.756915
96.484620	3299.206054	22.761933
96.140675	3310.928235	22.766951
96.324983	3307.782759	22.771968
96.332124	3321.394527	22.776986
96.561880	3334.451028	22.782003
96.937037	3326.536318	22.787021
97.077673	3330.353022	22.792039
97.246135	3328.395175	22.797056
97.150096	3328.053834	22.802074
97.197990	3325.880482	22.807091
97.459964	3324.916215	22.812109
97.275361	3325.980818	22.817127
97.444204	3323.445755	22.822144
97.458462	3345.904602	22.827162
97.653351	3359.446010	22.832179
97.992594	3359.666588	22.837197
97.690845	3364.585121	22.842215
98.131622	3370.882112	22.847232
98.220486	3357.864005	22.852250
97.929290	3363.389443	22.857267
98.387788	3359.594724	22.862285
98.236979	3357.172710	22.867303
98.301017	3369.480656	22.872320
98.541562	3384.868051	22.877338
98.289732	3383.892228	22.882355
98.444644	3384.593651	22.887373
98.595220	3392.980694	22.892391
98.881279	3407.713751	22.897408
99.083035	3412.130208	22.902426
98.694887	3413.255616	22.907443
99.149270	3411.548538	22.912461
99.249076	3399.986044	22.917479
99.130909	3413.380414	22.922496
99.572283	3432.821219	22.927514
99.231115	3444.157614	22.932531
99.583269	3432.322298	22.937549
99.526389	3438.879501	22.942567
99.758112	3438.589115	22.947584
99.997402	3461.146375	22.952602
100.039904	3468.580857	22.957619
100.325264	3467.460751	22.962637
100.532226	3469.736628	22.967655
100.850411	3466.762303	22.972672
100.908136	3455.760258	22.977690
100.741236	3462.234864	22.982707
100.864191	3460.286094	22.987725
100.810159	3466.198358	22.992743
101.125287	3449.661728	22.997760
101.112367	3455.365229	23.002778
101.051389	3453.448035	23.007795
101.207721	3476.898148	23.012813
101.143459	3479.955449	23.017831
101.208007	3485.428840	23.022848
101.430305	3486.015591	23.027866
101.101807	3492.353135	23.032883
101.741884	3480.617055	23.037901
101.887421	3491.696291	23.042919
101.904457	3508.350255	23.047936
101.998367	3510.831825	23.052954
102.019637	3508.940796	23.057971
102.159973	3519.761072	23.062989
102.141718	3519.822618	23.068007
102.456244	3519.044930	23.073024
102.510481	3513.009516	23.078042
102.202292	3519.374030	23.083059
102.709709	3534.841884	23.088077
102.936466	3536.336160	23.093095
102.923524	3545.106208	23.098112
102.826989	3542.638976	23.103130
103.055415	3543.200701	23.108147
103.333866	3541.543154	23.113165
103.642222	3562.724987	23.118183
103.504154	3569.719280	23.123200
103.742141	3566.808975	23.128218
103.926953	3574.563691	23.133235
103.836621	3559.343937	23.138253
103.946911	3563.980668	23.143271
103.948483	3553.951605	23.148288
104.220739	3558.650942	23.153306
103.759188	3553.348375	23.158323
103.950327	3560.454012	23.163341
104.221693	3569.532997	23.168359
104.256543	3589.681722	23.173376
104.717195	3577.220497	23.178394
104.469148	3573.054291	23.183411
104.852263	3587.102982	23.188429
104.749436	3599.273723	23.193447
104.927189	3605.115062	23.198464
104.721965	3606.448838	23.203482
105.028631	3606.893307	23.208499
105.000474	3607.752943	23.213517
105.214726	3625.645700	23.218535
105.248112	3639.393567	23.223552
105.541825	3635.366563	23.228570
105.506126	3634.247136	23.233587
105.795807	3652.448719	23.238605
105.763810	3660.083399	23.243623
105.893033	3656.144987	23.248640
106.493873	3660.474705	23.253658
106.143941	3662.244995	23.258675
106.231400	3669.715452	23.263693
106.620459	3681.627419	23.268711
106.653436	3698.069897	23.273728
106.929381	3686.172966	23.278746
106.710966	3687.219163	23.283763
106.881706	3690.444368	23.288781
107.158197	3684.264288	23.293799
107.326409	3685.733607	23.298816
107.359792	3682.888192	23.303834
107.339757	3690.114610	23.308851
107.452741	3705.675764	23.313869
107.676827	3703.087811	23.318887
107.881909	3720.036915	23.323904
108.005707	3720.330501	23.328922
107.947431	3722.134888	23.333939
108.084825	3716.034473	23.338957
108.266831	3708.256212	23.343975
108.243348	3714.002498	23.348992
108.367156	3715.558686	23.354010
108.043455	3720.991983	23.359027
108.477450	3736.965874	23.364045
108.918695	3731.263672	23.369063
108.545554	3743.930770	23.374080
108.852399	3734.539733	23.379098
108.945476	3738.607312	23.384115
108.909006	3745.039223	23.389133
108.920507	3739.277320	23.394151
109.098872	3768.299852	23.399168
109.555620	3768.796692	23.404186
109.477467	3783.799740	23.409203
109.354437	3776.141535	23.414221
109.217756	3770.493477	23.419239
109.051125	3790.432839	23.424256
109.670802	3791.137800	23.429274
109.707430	3800.294292	23.434291
109.910309	3804.942962	23.439309
110.052964	3823.433216	23.444327
110.130616	3830.284499	23.449344
110.550265	3830.814637	23.454362
110.798139	3836.082266	23.459379
110.580537	3829.344396	23.464397
110.726953	3828.570457	23.469415
110.662816	3845.159848	23.474432
111.240198	3852.975821	23.479450
111.300065	3857.248134	23.484467
111.327532	3862.248645	23.489485
111.398678	3849.910621	23.494503
111.134441	3847.593888	23.499520
111.108492	3863.621470	23.504538
111.617127	3876.326831	23.509555
111.728942	3886.959554	23.514573
112.158528	3874.994178	23.519591
111.954540	3888.646448	23.524608
112.008599	3889.907087	23.529626
112.381409	3896.772620	23.534643
112.195393	3914.316883	23.539661
112.597240	3903.521836	23.544679
112.750214	3917.712794	23.549696
112.532164	3912.926568	23.554714
112.785309	3920.267011	23.559731
112.837686	3942.592073	23.564749
113.174982	3936.711301	23.569767
113.167399	3943.425927	23.574784
113.354945	3931.091834	23.579802
113.204869	3934.561837	23.584819
113.248575	3947.679126	23.589837
113.859944	3955.248587	23.594855
113.871678	3966.212473	23.599872
113.947174	3973.460246	23.604890
114.123134	3974.851934	23.609907
114.001966	3963.090098	23.614925
114.258223	3946.885510	23.619943
114.215597	3961.365132	23.624960
114.645474	3973.708384	23.629978
114.581202	3993.053521	23.634995
114.689647	3988.845619	23.640013
114.830665	3988.433989	23.645031
114.866194	3999.736494	23.650048
115.272293	3985.380375	23.655066
114.960959	3992.645619	23.660083
115.146657	3988.221404	23.665101
115.272020	3996.687745	23.670119
115.242370	4009.382553	23.675136
115.941417	4006.698351	23.680154
115.960009	4010.623975	23.685171
116.115011	4001.955521	23.690189
116.118141	3998.182744	23.695207
116.030460	4014.370685	23.700224
116.355039	4005.900592	23.705242
116.215180	4004.101484	23.710259
116.047715	4008.057064	23.715277
116.635795	4014.536283	23.720295
116.643842	4029.332013	23.725312
116.948818	4024.388460	23.730330
116.875214	4028.184831	23.735347
116.316006	4029.060980	23.740365
116.881990	4023.210893	23.745383
116.867061	4045.205878	23.750400
116.939747	4048.252866	23.755418
116.824914	4055.461653	23.760435
116.707808	4068.666642	23.765453
116.898539	4084.233833	23.770471
116.917193	4092.374542	23.775488
117.521525	4098.015655	23.780506
117.996564	4112.492953	23.785523
118.115642	4113.405456	23.790541
118.235937	4113.112999	23.795559
118.443145	4132.288249	23.800576
118.441880	4143.635129	23.805594
118.345991	4143.206734	23.810611
118.424258	4149.929706	23.815629
119.103621	4141.177287	23.820647
118.899953	4146.510579	23.825664
119.047482	4155.074921	23.830682
119.567993	4151.577651	23.835699
119.522111	4163.328386	23.840717
119.630069	4167.045182	23.845735
119.729062	4170.459120	23.850752
119.849744	4168.783482	23.855770
119.959156	4161.357946	23.860787
119.867978	4166.719510	23.865805
119.976684	4155.895953	23.870823
120.094649	4177.171111	23.875840
120.237071	4191.399497	23.880858
120.480429	4192.836369	23.885875
120.512668	4210.402777	23.890893
120.416714	4200.494534	23.895911
120.874041	4198.404986	23.900928
120.711326	4212.394826	23.905946
121.096389	4217.164703	23.910963
120.898278	4228.440624	23.915981
120.994347	4225.431597	23.920999
121.175055	4228.098947	23.926016
121.440740	4248.383617	23.931034
121.560376	4258.670013	23.936051
121.430166	4262.036407	23.941069
121.722607	4255.508572	23.946087
121.831163	4262.630146	23.951104
121.966535	4273.176166	23.956122
122.166789	4266.023377	23.961139
122.271266	4282.200318	23.966157
122.431924	4278.856579	23.971175
122.706463	4279.183933	23.976192
122.924952	4296.438943	23.981210
123.132495	4294.205610	23.986227
123.504059	4309.539594	23.991245
123.359037	4303.582865	23.996263
123.601599	4304.955703	24.001280
123.331414	4302.523343	24.006298
123.341145	4289.388394	24.011315
123.490446	4301.178639	24.016333
123.892732	4300.772650	24.021351
123.801377	4307.835936	24.026368
123.687505	4296.341944	24.031386
123.958211	4319.240157	24.036403
124.103847	4333.072062	24.041421
124.134953	4318.677203	24.046439
124.669034	4322.735846	24.051456
124.408744	4322.070033	24.056474
124.217635	4328.478129	24.061491
124.458820	4345.028232	24.066509
124.871882	4347.610751	24.071527
125.069409	4357.523696	24.076544
124.835830	4362.515926	24.081562
125.231845	4363.953181	24.086579
125.125764	4386.623975	24.091597
125.466059	4387.728692	24.096615
125.360838	4390.101569	24.101632
125.517684	4390.142846	24.106650
125.684853	4405.511093	24.111667
125.781586	4419.536598	24.116685
126.328550	4410.947646	24.121703
126.446896	4412.500082	24.126720
126.404745	4415.402725	24.131738
126.571445	4412.806815	24.136755
126.587261	4417.588159	24.141773
126.911524	4433.569877	24.146791
126.790567	4427.380372	24.151808
127.144803	4424.925527	24.156826
127.429625	4425.326780	24.161843
126.988292	4430.638019	24.166861
127.472470	4441.684026	24.171879
127.685619	4453.631955	24.176896
127.779902	4451.737409	24.181914
127.875964	4450.021713	24.186931
128.224662	4448.460344	24.191949
128.361881	4449.512003	24.196967
127.870733	4450.005253	24.201984
127.895578	4462.815448	24.207002
128.240671	4475.654237	24.212019
128.260033	4484.480503	24.217037
128.442288	4495.989845	24.222055
128.941784	4507.936959	24.227072
128.481422	4514.617193	24.232090
128.707157	4510.050775	24.237107
128.946653	4528.213251	24.242125
129.205472	4541.360066	24.247143
129.451789	4540.886927	24.252160
129.448741	4543.763052	24.257178
129.653439	4554.950207	24.262195
129.974105	4572.880412	24.267213
130.315637	4562.547266	24.272231
130.625376	4570.538547	24.277248
130.367384	4577.070794	24.282266
130.575573	4564.294183	24.287283
130.430462	4562.453748	24.292301
130.634510	4571.914546	24.297319
130.872940	4597.920257	24.302336
130.883788	4603.365905	24.307354
131.334419	4590.553542	24.312371
131.034472	4601.750885	24.317389
131.191711	4594.500717	24.322407
131.342349	4606.669734	24.327424
131.518117	4629.449830	24.332442
131.514276	4620.756491	24.337459
131.605442	4625.504581	24.342477
131.620931	4634.932790	24.347495
131.959240	4637.629685	24.352512
132.106720	4657.298947	24.357530
132.560414	4641.765785	24.362547
132.167540	4657.437858	24.367565
132.401497	4665.960246	24.372583
132.644008	4674.454452	24.377600
132.581743	4674.308300	24.382618
132.999789	4675.595873	24.387635
133.159144	4683.500636	24.392653
133.362110	4705.939714	24.397671
133.319764	4706.102102	24.402688
133.442692	4711.094199	24.407706
133.594122	4720.949635	24.412723
133.528581	4728.162398	24.417741
133.502683	4727.347199	24.422759
134.101923	4733.452019	24.427776
134.098929	4747.259635	24.432794
134.164798	4744.843729	24.437811
134.354820	4745.074422	24.442829
134.566675	4755.323466	24.447847
134.828829	4758.803099	24.452864
135.012160	4769.810068	24.457882
135.282165	4763.629849	24.462899
135.052474	4761.910460	24.467917
135.016906	4769.202154	24.472935
135.480986	4779.608370	24.477952
135.443831	4795.849801	24.482970
135.693601	4794.788246	24.487987
135.429481	4794.471101	24.493005
135.759799	4806.573968	24.498023
136.180443	4820.537650	24.503040
135.882277	4824.235483	24.508058
136.131623	4817.431838	24.513075
136.348167	4834.308603	24.518093
136.287206	4854.533462	24.523111
136.892507	4847.319385	24.528128
136.799374	4861.376660	24.533146
137.163910	4863.460948	24.538163
137.254126	4872.047755	24.543181
137.561244	4881.155463	24.548199
137.457542	4868.124210	24.553216
137.516569	4878.791925	24.558234
137.411995	4872.988542	24.563251
137.815189	4884.186840	24.568269
137.744456	4902.934519	24.573287
137.741584	4891.813904	24.578304
137.925597	4918.395328	24.583322
138.516071	4923.279527	24.588339
138.673366	4934.631887	24.593357
138.604182	4938.899834	24.598375
139.123946	4934.070913	24.603392
138.999636	4957.053052	24.608410
138.997014	4963.592480	24.613427
139.678173	4961.820210	24.618445
139.552409	4956.673895	24.623463
139.622328	4955.467230	24.628480
140.115942	4958.338537	24.633498
140.255483	4954.450067	24.638515
139.982861	4958.863455	24.643533
140.032232	4976.019987	24.648551
140.527047	4977.072836	24.653568
140.358780	4970.714145	24.658586
140.544309	4976.964594	24.663603
140.699166	4963.918493	24.668621
140.788689	4990.638104	24.673639
141.008871	4997.064347	24.678656
141.085683	4995.473436	24.683674
141.204886	5006.437228	24.688691
141.331311	5004.383748	24.693709
141.501034	5035.381892	24.698727
141.936318	5026.070051	24.703744
141.631675	5037.330689	24.708762
141.935950	5040.382130	24.713779
142.045285	5040.916343	24.718797
141.937531	5046.950691	24.723815
141.846378	5062.313840	24.728832
141.880689	5074.513863	24.733850
142.025838	5074.582670	24.738867
142.245691	5094.279504	24.743885
142.510495	5102.700964	24.748903
142.687429	5097.713266	24.753920
143.081985	5122.337237	24.758938
143.109577	5122.847556	24.763955
143.470479	5125.988878	24.768973
143.328297	5133.421204	24.773991
143.509395	5143.836231	24.779008
143.957612	5149.577552	24.784026
144.064592	5150.489754	24.789043
144.083926	5154.412787	24.794061
143.988330	5175.708058	24.799079
144.135824	5172.704921	24.804096
144.558085	5178.345019	24.809114
144.639584	5180.510374	24.814131
145.311904	5198.389887	24.819149
145.336476	5214.651084	24.824167
145.735556	5204.333995	24.829184
145.572211	5198.651236	24.834202
145.701784	5200.773213	24.839219
145.836276	5208.532336	24.844237
145.717707	5211.633205	24.849255
145.942132	5219.622379	24.854272
146.066872	5229.227403	24.859290
146.072034	5236.425174	24.864307
146.256840	5241.704885	24.869325
146.216841	5249.002260	24.874343
146.437565	5260.524710	24.879360
147.000718	5266.299450	24.884378
146.879173	5259.222612	24.889395
147.146321	5283.100095	24.894413
147.167778	5290.831868	24.899431
147.459302	5299.487627	24.904448
147.406395	5300.162449	24.909466
147.739352	5303.671849	24.914483
147.934046	5301.476722	24.919501
148.264200	5316.738220	24.924519
148.427284	5315.343280	24.929536
148.800000	5311.298072	24.934554
148.631950	5312.420312	24.939571
148.691449	5310.883810	24.944589
148.624599	5323.423218	24.949607
148.885863	5338.022032	24.954624
149.001475	5341.663427	24.959642
149.156880	5356.054528	24.964659
149.281571	5350.092206	24.969677
149.245145	5373.048228	24.974695
149.231076	5378.892007	24.979712
149.228602	5383.451054	24.984730
149.469077	5405.443946	24.989747
149.690327	5406.436899	24.994765
149.733024	5423.973807	24.999783
150.452471	5428.750234	25.004800
150.228997	5438.654288	25.009818
150.481162	5461.614729	25.014835
150.741898	5459.456312	25.019853
150.711842	5471.003817	25.024871
150.930230	5469.950948	25.029888
151.147017	5490.162627	25.034906
151.596148	5502.691732	25.039923
151.902451	5489.765462	25.044941
151.847128	5500.802538	25.049959
151.925879	5491.490665	25.054976
152.311009	5509.518002	25.059994
152.257941	5521.607994	25.065011
152.771793	5521.969073	25.070029
152.898089	5521.081041	25.075047
152.771990	5518.503011	25.080064
152.858292	5518.824487	25.085082
152.871300	5532.813245	25.090099
152.927133	5526.935864	25.095117
152.982588	5535.040532	25.100135
153.050921	5548.858726	25.105152
153.375018	5559.105897	25.110170
153.210226	5557.039434	25.115187
153.542895	5569.784317	25.120205
153.621730	5584.932860	25.125223
153.981400	5590.454696	25.130240
154.128199	5608.951896	25.135258
154.171216	5621.216663	25.140275
154.445853	5616.523720	25.145293
154.279972	5632.390388	25.150311
154.772578	5641.962444	25.155328
155.066344	5637.024571	25.160346
155.208434	5665.532546	25.165363
155.438977	5666.826382	25.170381
155.670621	5666.771438	25.175399
155.516676	5679.877954	25.180416
155.702214	5679.115969	25.185434
155.739138	5702.687994	25.190451
155.850703	5690.915930	25.195469
156.069283	5717.520170	25.200487
156.121383	5728.316398	25.205504
156.594538	5734.001053	25.210522
156.518307	5745.583166	25.215539
157.002569	5748.491212	25.220557
157.035888	5754.056792	25.225575
156.978955	5766.573259	25.230592
157.393312	5778.809473	25.235610
157.621352	5787.731539	25.240627
157.870337	5780.086479	25.245645
157.730999	5787.342636	25.250663
157.899728	5799.120565	25.255680
158.491750	5802.403784	25.260698
158.467301	5808.007673	25.265715
158.859271	5811.543270	25.270733
158.729562	5813.788499	25.275751
159.228310	5827.963832	25.280768
159.302146	5828.340137	25.285786
159.226913	5843.037549	25.290803
159.955888	5841.262406	25.295821
159.794147	5842.548231	25.300839
159.674411	5838.301935	25.305856
160.130785	5852.344115	25.310874
159.853406	5866.950130	25.315891
159.775648	5873.659856	25.320909
160.260993	5863.763971	25.325927
160.164737	5888.441504	25.330944
160.363241	5892.468601	25.335962
160.017870	5916.215153	25.340979
160.388742	5922.187684	25.345997
160.629697	5930.066208	25.351015
160.747245	5967.189880	25.356032
161.316462	5963.212053	25.361050
161.252151	5984.510340	25.366067
161.504001	6004.142001	25.371085
162.092220	5993.888435	25.376103
162.018355	6007.150915	25.381120
162.060153	6017.114273	25.386138
162.278100	6036.549184	25.391155
162.651260	6021.339827	25.396173
162.768533	6044.831362	25.401191
162.664650	6045.779640	25.406208
163.099104	6055.050488	25.411226
163.079388	6059.868919	25.416243
163.420428	6062.834554	25.421261
163.269513	6065.751535	25.426279
163.366854	6076.816948	25.431296
163.662901	6081.217801	25.436314
163.879492	6083.870880	25.441331
164.018293	6093.904887	25.446349
164.535422	6109.311883	25.451367
164.414562	6117.781471	25.456384
164.944185	6114.738641	25.461402
164.719742	6120.813157	25.466419
164.724823	6130.848806	25.471437
165.294914	6145.843874	25.476455
165.222369	6152.952527	25.481472
165.534805	6141.627721	25.486490
165.542584	6157.952916	25.491507
165.827923	6173.955057	25.496525
165.894779	6175.490977	25.501543
166.240354	6181.492595	25.506560
166.605213	6180.150475	25.511578
166.257102	6203.559276	25.516595
166.244616	6202.852037	25.521613
166.565457	6208.652207	25.526631
166.850730	6230.503401	25.531648
166.999119	6235.754027	25.536666
166.596667	6245.062468	25.541683
166.848360	6252.492456	25.546701
167.332263	6258.063305	25.551719
167.425950	6282.332450	25.556736
167.535098	6286.687852	25.561754
168.176974	6316.828890	25.566771
168.441983	6315.422142	25.571789
168.456348	6327.038540	25.576807
168.451357	6323.117700	25.581824
168.969930	6343.064043	25.586842
168.996271	6355.854276	25.591859
168.992412	6355.645692	25.596877
168.893337	6360.320607	25.601895
169.163356	6376.391639	25.606912
169.504666	6383.277656	25.611930
169.587662	6399.637927	25.616947
169.862796	6405.087391	25.621965
170.113566	6412.486894	25.626983
170.147695	6435.510778	25.632000
170.535606	6434.379040	25.637018
170.691636	6448.973440	25.642035
170.785292	6458.284300	25.647053
171.378314	6465.709182	25.652071
171.088770	6480.196887	25.657088
171.356779	6478.563604	25.662106
171.620001	6499.510778	25.667123
171.896550	6503.619643	25.672141
172.106392	6497.354970	25.677159
171.990951	6495.370007	25.682176
172.284159	6510.003226	25.687194
172.301017	6533.968861	25.692212
172.446662	6535.241359	25.697229
172.537793	6542.152246	25.702247
172.607128	6568.834174	25.707264
172.884131	6559.645240	25.712282
173.096391	6581.809830	25.717300
173.451305	6582.147587	25.722317
173.739817	6590.488359	25.727335
173.787084	6594.565828	25.732352
174.000915	6613.394145	25.737370
174.069450	6620.693912	25.742388
174.350036	6620.607648	25.747405
174.188320	6629.497725	25.752423
174.474107	6636.220555	25.757440
174.871455	6651.623464	25.762458
175.108717	6655.071804	25.767476
174.831413	6647.971639	25.772493
175.164120	6673.339119	25.777511
175.393216	6671.278304	25.782528
176.013949	6670.431766	25.787546
175.924263	6679.395025	25.792564
175.826619	6700.735229	25.797581
176.272339	6706.080220	25.802599
176.225835	6706.140145	25.807616
176.254843	6710.100165	25.812634
176.445541	6727.740871	25.817652
176.540669	6732.750022	25.822669
176.871903	6750.774700	25.827687
176.929208	6763.594801	25.832704
177.255239	6759.006438	25.837722
177.728908	6789.231307	25.842740
177.806708	6792.393364	25.847757
178.061311	6790.490557	25.852775
178.012723	6804.085031	25.857792
178.373403	6814.542772	25.862810
178.412395	6826.849311	25.867828
178.591824	6829.152681	25.872845
179.128459	6848.127984	25.877863
178.977512	6845.483353	25.882880
179.646778	6847.604983	25.887898
179.727218	6855.871593	25.892916
179.935265	6872.937038	25.897933
180.297559	6875.207050	25.902951
179.915959	6874.430822	25.907968
180.180183	6885.418827	25.912986
180.463367	6878.537824	25.918004
180.589713	6896.925724	25.923021
180.662366	6901.662995	25.928039
180.513497	6907.844247	25.933056
180.855654	6927.533023	25.938074
181.062749	6937.421611	25.943092
181.111805	6937.514576	25.948109
181.444325	6951.049357	25.953127
181.119315	6972.464512	25.958144
181.814490	6990.111154	25.963162
182.033125	6993.216116	25.968180
182.298288	7006.778614	25.973197
182.686793	7023.312723	25.978215
183.018768	7033.686358	25.983232
182.733378	7032.590222	25.988250
183.260592	7035.361469	25.993268
183.306210	7051.201707	25.998285
183.607361	7065.647478	26.003303
183.375072	7065.209640	26.008320
183.889680	7073.351860	26.013338
183.803510	7083.848172	26.018356
183.600973	7094.855953	26.023373
184.100404	7102.202095	26.028391
184.163361	7122.589359	26.033408
184.370154	7134.220237	26.038426
184.826993	7145.586925	26.043444
184.502146	7168.023017	26.048461
184.857842	7172.959327	26.053479
185.188836	7190.894765	26.058496
185.522378	7196.506548	26.063514
185.615707	7202.493531	26.068532
185.692783	7215.861251	26.073549
186.341871	7226.399990	26.078567
186.358186	7247.200725	26.083584
186.565517	7241.732418	26.088602
186.566723	7248.220578	26.093620
186.668088	7259.757920	26.098637
187.089286	7272.919976	26.103655
186.847942	7283.160105	26.108672
187.265597	7290.033909	26.113690
187.503988	7309.043296	26.118708
187.855316	7315.019197	26.123725
187.804051	7327.237078	26.128743
187.854558	7343.017732	26.133760
187.881644	7344.465829	26.138778
188.316348	7366.869638	26.143796
188.480061	7374.958943	26.148813
189.008449	7394.022115	26.153831
189.147493	7400.686823	26.158848
189.257072	7407.284732	26.163866
189.777641	7414.726765	26.168884
189.742012	7424.968438	26.173901
190.291294	7427.071383	26.178919
190.270180	7423.626276	26.183936
190.563462	7421.750083	26.188954
190.660273	7434.440549	26.193972
190.569198	7445.658558	26.198989
191.354998	7458.112340	26.204007
191.561160	7445.322702	26.209024
191.551448	7453.342253	26.214042
191.933551	7454.539528	26.219060
191.860967	7485.804253	26.224077
192.048331	7476.746163	26.229095
192.277103	7475.529599	26.234112
192.075597	7487.514885	26.239130
192.613882	7501.820276	26.244148
192.276137	7509.604221	26.249165
192.662595	7525.922609	26.254183
192.921431	7540.474257	26.259200
193.071929	7550.069357	26.264218
193.014540	7555.116571	26.269236
192.995041	7573.812894	26.274253
193.493415	7592.225985	26.279271
193.527527	7606.183170	26.284288
193.847505	7630.296498	26.289306
193.856354	7635.105177	26.294324
194.109549	7662.518611	26.299341
195.107100	7656.768377	26.304359
195.245233	7676.319315	26.309376
195.209236	7681.368548	26.314394
196.011701	7686.012249	26.319412
196.085222	7683.056302	26.324429
196.035696	7683.374276	26.329447
196.171509	7688.395911	26.334464
196.125011	7694.983499	26.339482
196.677265	7706.189122	26.344500
196.785639	7717.175893	26.349517
196.915978	7714.045155	26.354535
197.053120	7731.266590	26.359552
197.212509	7745.600940	26.364570
197.465318	7749.494314	26.369588
197.421775	7753.201160	26.374605
197.536282	7766.393826	26.379623
197.641714	7787.267972	26.384640
197.890089	7792.611289	26.389658
198.075449	7805.921450	26.394676
198.121724	7819.497185	26.399693
198.566307	7830.167785	26.404711
198.723839	7844.603346	26.409728
198.890875	7852.782923	26.414746
199.332898	7866.058602	26.419764
199.170968	7879.229302	26.424781
199.706556	7872.584981	26.429799
199.841088	7886.578592	26.434816
199.517875	7916.716759	26.439834
200.207073	7909.202720	26.444852
200.067559	7931.045337	26.449869
200.499995	7937.931948	26.454887
200.523437	7952.408665	26.459904
200.661100	7972.838240	26.464922
200.986663	7975.097945	26.469940
201.188073	7998.588731	26.474957
201.383647	7994.513831	26.479975
201.720786	8006.701930	26.484992
201.737147	8025.041582	26.490010
202.189108	8018.479541	26.495028
202.508556	8035.597937	26.500045
202.579058	8055.744146	26.505063
202.937064	8068.896832	26.510080
202.938033	8076.543964	26.515098
203.376166	8080.717912	26.520116
203.597295	8102.283793	26.525133
203.789755	8093.029179	26.530151
203.960027	8116.755272	26.535168
204.068227	8130.408469	26.540186
204.642474	8114.078532	26.545204
204.076901	8143.160013	26.550221
204.046855	8154.520451	26.555239
204.575887	8167.255087	26.560256
204.865355	8172.791801	26.565274
204.853141	8190.032112	26.570292
205.110425	8211.756783	26.575309
205.388103	8220.306571	26.580327
205.985975	8233.186624	26.585344
205.809983	8251.045572	26.590362
206.408239	8263.185212	26.595380
206.787210	8279.240186	26.600397
206.952658	8279.617955	26.605415
207.313749	8294.818954	26.610432
207.192231	8310.307642	26.615450
207.702134	8303.171965	26.620468
207.747425	8328.463576	26.625485
208.042781	8337.065641	26.630503
208.030546	8341.722066	26.635520
208.101775	8352.466522	26.640538
208.298513	8368.998286	26.645556
208.756278	8371.554412	26.650573
208.695172	8384.781335	26.655591
208.774968	8398.196076	26.660608
208.885957	8421.363744	26.665626
209.273657	8430.749270	26.670644
209.088441	8445.809899	26.675661
209.343393	8466.445997	26.680679
209.940248	8484.401204	26.685696
210.014688	8513.439838	26.690714
210.452790	8520.564426	26.695732
210.618856	8532.148717	26.700749
210.869225	8537.373812	26.705767
211.372436	8557.642138	26.710784
211.021856	8562.779072	26.715802
211.292811	8571.310470	26.720820
211.128391	8595.582495	26.725837
211.718619	8613.367236	26.730855
212.215340	8623.351594	26.735872
212.138389	8647.168949	26.740890
212.182619	8654.106626	26.745908
212.557649	8666.731635	26.750925
212.879983	8690.207405	26.755943
213.378980	8688.443581	26.760960
213.696339	8698.698643	26.765978
213.872813	8716.237589	26.770996
214.255558	8723.086284	26.776013
214.270401	8720.892050	26.781031
214.549233	8722.127758	26.786048
214.547056	8741.088034	26.791066
214.559974	8752.510328	26.796084
214.997691	8757.202017	26.801101
214.980990	8779.643820	26.806119
215.577909	8780.124385	26.811136
215.429868	8792.191614	26.816154
215.628355	8802.572717	26.821172
215.950474	8815.044328	26.826189
215.857483	8819.083321	26.831207
216.225972	8839.234851	26.836224
215.885855	8857.568201	26.841242
216.543402	8873.198097	26.846260
217.270767	8883.023999	26.851277
216.783252	8913.711060	26.856295
217.239658	8911.975517	26.861312
217.567538	8940.956517	26.866330
218.078527	8948.833293	26.871348
218.242999	8959.330393	26.876365
218.331820	8977.765509	26.881383
218.878973	8976.688421	26.886400
218.760496	9004.487744	26.891418
218.969185	9005.805166	26.896436
219.453338	9020.810093	26.901453
219.119294	9039.516003	26.906471
219.966401	9036.265793	26.911488
219.922372	9051.881030	26.916506
220.149720	9059.905547	26.921524
220.798021	9075.675802	26.926541
220.514898	9093.085517	26.931559
221.339771	9097.501457	26.936576
221.183166	9107.843759	26.941594
221.467176	9118.340118	26.946612
221.625216	9130.763471	26.951629
221.448710	9133.405615	26.956647
221.642355	9153.849517	26.961664
221.941540	9170.103681	26.966682
222.282309	9188.834540	26.971700
222.724692	9185.528293	26.976717
222.860507	9204.155977	26.981735
223.418598	9207.770060	26.986752
223.477567	9220.970750	26.991770
223.859305	9237.685527	26.996788
224.136871	9244.217851	27.001805
224.377709	9260.081606	27.006823
224.562591	9252.281632	27.011840
224.306646	9277.217293	27.016858
224.444120	9283.271813	27.021876
224.705893	9296.166519	27.026893
224.743471	9308.078228	27.031911
225.052760	9319.893065	27.036928
225.276574	9349.573353	27.041946
225.517712	9368.340577	27.046964
226.235538	9379.261676	27.051981
225.998859	9398.321345	27.056999
226.553363	9408.665291	27.062016
226.415435	9429.033574	27.067034
226.666555	9438.107497	27.072052
227.285399	9448.557417	27.077069
227.051386	9457.026215	27.082087
227.475483	9470.106132	27.087104
227.782604	9504.058776	27.092122
227.751274	9500.749601	27.097140
228.117863	9509.286972	27.102157
228.194271	9536.795872	27.107175
228.580378	9548.344550	27.112192
228.840246	9549.601575	27.117210
229.175225	9563.869961	27.122228
229.371464	9579.439716	27.127245
229.423657	9584.382034	27.132263
230.132714	9599.672519	27.137280
230.177325	9607.318690	27.142298
230.234560	9622.192284	27.147316
230.342013	9633.491676	27.152333
230.709918	9647.070973	27.157351
231.013230	9654.542091	27.162368
231.398270	9687.842640	27.167386
231.191037	9693.581686	27.172404
231.218569	9691.967335	27.177421
231.486908	9723.199827	27.182439
231.877632	9728.084682	27.187456
232.266497	9742.495565	27.192474
232.198211	9768.184753	27.197492
232.777530	9771.467774	27.202509
232.819341	9799.490915	27.207527
233.095328	9802.208860	27.212544
233.598809	9822.492151	27.217562
233.748179	9843.596478	27.222580
234.470412	9842.465204	27.227597
233.950582	9871.409150	27.232615
234.334976	9872.477057	27.237632
234.496998	9893.419454	27.242650
234.560726	9908.361561	27.247668
234.799040	9924.239786	27.252685
234.822876	9946.115681	27.257703
235.177796	9953.349976	27.262720
234.914362	9988.171456	27.267738
235.752265	10011.286719	27.272756
236.228124	10027.114772	27.277773
236.145370	10044.534954	27.282791
236.836454	10065.537469	27.287808
237.456369	10079.214137	27.292826
237.369129	10092.249865	27.297844
237.401074	10098.007830	27.302861
237.569924	10113.242335	27.307879
238.229177	10134.883531	27.312896
238.397589	10142.477995	27.317914
238.582438	10155.355387	27.322932
238.928320	10162.080036	27.327949
239.247135	10188.732350	27.332967
239.511024	10184.239929	27.337984
239.925242	10197.960926	27.343002
240.017332	10198.683286	27.348020
240.690800	10205.032437	27.353037
240.779513	10205.601749	27.358055
240.787623	10214.249143	27.363072
241.124660	10230.229522	27.368090
241.160839	10233.406235	27.373108
241.402147	10230.546557	27.378125
241.263287	10253.907054	27.383143
241.685009	10270.001881	27.388160
241.632898	10282.681419	27.393178
241.553574	10296.818830	27.398196
242.275892	10324.520135	27.403213
242.173005	10338.259731	27.408231
242.427749	10349.707809	27.413248
242.768552	10382.029297	27.418266
243.169846	10400.649966	27.423284
243.577656	10418.822144	27.428301
243.644661	10441.741641	27.433319
243.671497	10449.491984	27.438336
244.137166	10462.742305	27.443354
244.241554	10483.810796	27.448372
244.777883	10494.950138	27.453389
245.221455	10498.078500	27.458407
245.579069	10518.515968	27.463424
245.977064	10524.573607	27.468442
245.831938	10530.746190	27.473460
246.192217	10541.876840	27.478477
246.201627	10562.772069	27.483495
246.338691	10573.309423	27.488512
246.681612	10585.184240	27.493530
246.284196	10607.659217	27.498548
246.973138	10621.269806	27.503565
247.159218	10636.451548	27.508583
247.448293	10658.031727	27.513600
247.614016	10672.589030	27.518618
247.729745	10699.798818	27.523636
248.080636	10702.796799	27.528653
248.277255	10725.014669	27.533671
248.630657	10752.002519	27.538688
249.289311	10758.166067	27.543706
249.152011	10771.487908	27.548724
249.642845	10781.455696	27.553741
249.441363	10812.632448	27.558759
249.886157	10825.109003	27.563776
250.178186	10851.806237	27.568794
250.212508	10873.773836	27.573812
250.710271	10887.784912	27.578829
250.639755	10911.254815	27.583847
250.977161	10937.887976	27.588864
251.503467	10953.702314	27.593882
251.463449	10973.613661	27.598900
251.881690	10991.667391	27.603917
252.090161	11017.019808	27.608935
252.436164	11034.627040	27.613952
253.185227	11055.264423	27.618970
253.056066	11085.003103	27.623988
253.796128	11089.731405	27.629005
253.743594	11109.435441	27.634023
254.004443	11127.794988	27.639040
254.346575	11130.506173	27.644058
254.354278	11164.052544	27.649076
254.502182	11167.281883	27.654093
255.372876	11186.712163	27.659111
254.991907	11203.566833	27.664128
255.677765	11224.780502	27.669146
255.945044	11238.673987	27.674164
256.032271	11247.576712	27.679181
256.594640	11253.983244	27.684199
256.517252	11273.644320	27.689216
256.930060	11286.052469	27.694234
256.821299	11306.763368	27.699252
257.270193	11325.519052	27.704269
257.498886	11332.703929	27.709287
257.541607	11367.347836	27.714304
258.136006	11382.900833	27.719322
258.272069	11396.727114	27.724340
258.492227	11419.561258	27.729357
258.929730	11445.998324	27.734375
258.894923	11464.400802	27.739392
259.285391	11473.285851	27.744410
259.370762	11494.428926	27.749428
259.539768	11504.670920	27.754445
260.122554	11520.098348	27.759463
260.178590	11543.355255	27.764480
261.218433	11549.364752	27.769498
260.847174	11568.740717	27.774516
261.241113	11591.384108	27.779533
261.986431	11600.504449	27.784551
261.556609	11605.571145	27.789568
262.404485	11622.248437	27.794586
262.466355	11634.591941	27.799604
262.567056	11650.082599	27.804621
262.622414	11667.020861	27.809639
262.624898	11672.533739	27.814656
263.216384	11686.936538	27.819674
263.238558	11712.779334	27.824692
263.482850	11724.297875	27.829709
263.497737	11747.282206	27.834727
263.808693	11767.704557	27.839744
264.424979	11783.518243	27.844762
264.230684	11807.932425	27.849780
264.790815	11824.322650	27.854797
265.001049	11847.668754	27.859815
265.604729	11866.454645	27.864832
265.834614	11875.204948	27.869850
265.949344	11913.376978	27.874868
266.231572	11922.218710	27.879885
267.065350	11941.920715	27.884903
266.940032	11969.017280	27.889920
267.159638	11970.660093	27.894938
267.233759	11993.200115	27.899956
267.640992	12004.031747	27.904973
268.118615	12026.750950	27.909991
268.330313	12043.892247	27.915008
268.705253	12059.723234	27.920026
268.892182	12075.414342	27.925044
268.865432	12098.861413	27.930061
269.280991	12111.302049	27.935079
269.697315	12127.537508	27.940096
270.268121	12159.253409	27.945114
270.214234	12180.841879	27.950132
270.299532	12187.088897	27.955149
270.728191	12207.963481	27.960167
270.853939	12231.844066	27.965184
271.247608	12245.507192	27.970202
271.678907	12263.664192	27.975220
271.632958	12271.307689	27.980237
272.193086	12299.563120	27.985255
272.231461	12313.481173	27.990272
272.570877	12329.311204	27.995290
272.867088	12365.391776	28.000308
272.780890	12369.954447	28.005325
273.635534	12390.044323	28.010343
273.619763	12400.371777	28.015360
274.261846	12427.319478	28.020378
274.291378	12446.649186	28.025396
274.368112	12473.862905	28.030413
274.992709	12480.978162	28.035431
274.785676	12501.990455	28.040448
275.370352	12526.618161	28.045466
275.713949	12546.826543	28.050484
275.670149	12564.792146	28.055501
276.204816	12588.030574	28.060519
276.401482	12599.845963	28.065536
276.736039	12624.488355	28.070554
276.877468	12638.356573	28.075572
276.953807	12668.088645	28.080589
277.417212	12681.558628	28.085607
277.760139	12710.457309	28.090624
278.257520	12719.742949	28.095642
278.284329	12728.501268	28.100660
278.657611	12770.366241	28.105677
279.133514	12780.084056	28.110695
279.169394	12801.621497	28.115712
279.599781	12810.806382	28.120730
279.634550	12831.310378	28.125748
279.681861	12842.556576	28.130765
280.492816	12857.801844	28.135783
280.785070	12884.881378	28.140800
280.960305	12882.364629	28.145818
281.316741	12906.624091	28.150836
281.422060	12929.037359	28.155853
282.061748	12940.808168	28.160871
282.231752	12953.728077	28.165888
282.302280	12975.652381	28.170906
282.640444	12983.344630	28.175924
282.717078	13002.888612	28.180941
283.121082	13011.800643	28.185959
283.261884	13038.610795	28.190976
283.809116	13059.304593	28.195994
283.945284	13074.603248	28.201012
284.055169	13098.569675	28.206029
284.372672	13112.168122	28.211047
284.625324	13137.431490	28.216064
284.767923	13158.485354	28.221082
285.308178	13188.319798	28.226100
285.610896	13206.430560	28.231117
285.966688	13220.497074	28.236135
286.135002	13246.048727	28.241152
286.236846	13263.028257	28.246170
286.895251	13280.500460	28.251188
287.181775	13305.096677	28.256205
287.737856	13315.918785	28.261223
287.651940	13348.482194	28.266240
288.096218	13350.555247	28.271258
288.320934	13376.452335	28.276276
288.345226	13398.295031	28.281293
288.870288	13410.425489	28.286311
288.972937	13434.815915	28.291328
289.149780	13461.190627	28.296346
289.930119	13478.154410	28.301364
289.632877	13512.152351	28.306381
290.120147	13526.107590	28.311399
290.519134	13555.909324	28.316416
290.780009	13572.243621	28.321434
291.135631	13598.729266	28.326452
291.102360	13623.106188	28.331469
291.944378	13628.438487	28.336487
292.356868	13664.951063	28.341504
292.629047	13687.810554	28.346522
292.974316	13705.700537	28.351540
293.134052	13720.614566	28.356557
293.677657	13733.273248	28.361575
293.594625	13763.860959	28.366592
293.910584	13778.708260	28.371610
294.507166	13801.539529	28.376628
294.555954	13812.154258	28.381645
295.139477	13823.457524	28.386663
295.285865	13842.459946	28.391680
295.570864	13862.359766	28.396698
295.614350	13877.012649	28.401716
295.751661	13905.933255	28.406733
296.113738	13934.320396	28.411751
296.214352	13951.894936	28.416768
296.639656	13975.400835	28.421786
296.919475	13992.287117	28.426804
297.393143	14021.770084	28.431821
297.723968	14035.356076	28.436839
298.149411	14054.982373	28.441856
298.437801	14071.509608	28.446874
298.499961	14086.151715	28.451892
298.969145	14118.442163	28.456909
299.197678	14132.667593	28.461927
299.671132	14146.825784	28.466944
299.576840	14172.100810	28.471962
300.335607	14182.518117	28.476980
300.851778	14192.518515	28.481997
301.090127	14210.730859	28.487015
301.240637	14223.495842	28.492032
301.160166	14232.302640	28.497050
301.668894	14258.857045	28.502068
301.766877	14269.876818	28.507085
301.688217	14286.324661	28.512103
302.307807	14324.351998	28.517120
302.583103	14342.834162	28.522138
302.782555	14357.666573	28.527156
303.021939	14386.459285	28.532173
303.254896	14413.325824	28.537191
304.212311	14435.977034	28.542208
304.092467	14451.705373	28.547226
304.724170	14465.642290	28.552244
304.700054	14487.650460	28.557261
305.370051	14504.290013	28.562279
305.480080	14522.949394	28.567296
305.705426	14552.723340	28.572314
305.830668	14561.754774	28.577332
306.358330	14590.963532	28.582349
306.410090	14618.653016	28.587367
307.037194	14642.126542	28.592384
307.106324	14679.612144	28.597402
307.419625	14696.290338	28.602420
307.667003	14716.975913	28.607437
308.273628	14745.440687	28.612455
308.463002	14777.950446	28.617472
308.555736	14795.492530	28.622490
308.994748	14815.695863	28.627508
309.305018	14848.797242	28.632525
309.599095	14873.036857	28.637543
310.115218	14889.866123	28.642560
310.148176	14928.626884	28.647578
310.650720	14944.460894	28.652596
311.021106	14978.844859	28.657613
311.313846	14996.325750	28.662631
311.759171	15024.554482	28.667648
312.259607	15043.588068	28.672666
312.433760	15053.944930	28.677684
312.556452	15083.628067	28.682701
312.851681	15096.223265	28.687719
313.223939	15117.712932	28.692736
313.502183	15147.895274	28.697754
314.167752	15167.782674	28.702772
314.534625	15195.837127	28.707789
314.399920	15221.128335	28.712807
314.580477	15248.633711	28.717824
314.704365	15274.588304	28.722842
315.308489	15288.664443	28.727860
315.545529	15325.192401	28.732877
315.851976	15353.559691	28.737895
316.623886	15369.266089	28.742912
316.490292	15399.264781	28.747930
317.143817	15414.566846	28.752948
317.192951	15446.560551	28.757965
317.586918	15470.169924	28.762983
318.171279	15499.344154	28.768000
318.033121	15515.801489	28.773018
318.855085	15538.621609	28.778036
318.927522	15567.910479	28.783053
319.388283	15584.766947	28.788071
319.816345	15606.104625	28.793088
319.979372	15626.460150	28.798106
320.488565	15647.447218	28.803124
320.521109	15665.586447	28.808141
320.695890	15693.862610	28.813159
320.937755	15708.870484	28.818176
321.258653	15735.653755	28.823194
321.924599	15752.621490	28.828212
322.173897	15775.865935	28.833229
322.632962	15790.032666	28.838247
323.056225	15806.350263	28.843264
323.081074	15834.232221	28.848282
323.348196	15848.211648	28.853300
323.541249	15884.127176	28.858317
323.654535	15904.741850	28.863335
324.476141	15928.309606	28.868352
324.726748	15953.412208	28.873370
324.919492	15964.067596	28.878388
325.079961	16003.329925	28.883405
325.124610	16023.905656	28.888423
325.913891	16041.324548	28.893440
325.992522	16074.818135	28.898458
326.543348	16096.517571	28.903476
326.394449	16141.864384	28.908493
326.819064	16157.266432	28.913511
327.404145	16191.953179	28.918528
327.398235	16223.290831	28.923546
328.275657	16233.273787	28.928564
328.501828	16280.867923	28.933581
328.611893	16299.338626	28.938599
328.829027	16318.114752	28.943616
329.339242	16368.119279	28.948634
329.714492	16383.375243	28.953652
330.321656	16421.376429	28.958669
330.252083	16438.261503	28.963687
330.946454	16471.988303	28.968704
330.829891	16502.216304	28.973722
331.705477	16519.005206	28.978740
331.875611	16548.908541	28.983757
332.121335	16570.080592	28.988775
333.095784	16596.106382	28.993792
333.080460	16626.046800	28.998810
333.635907	16648.294682	29.003828
333.832496	16666.565526	29.008845
334.008331	16688.792645	29.013863
334.520260	16710.814540	29.018880
334.814255	16745.638810	29.023898
335.183569	16767.829343	29.028916
335.599950	16783.755030	29.033933
335.746939	16809.577423	29.038951
336.290038	16820.820114	29.043968
336.264732	16849.422903	29.048986
336.784227	16874.056946	29.054004
337.325478	16905.206210	29.059021
337.488245	16921.987201	29.064039
337.953039	16940.485132	29.069056
338.088282	16965.887314	29.074074
338.319787	16994.553530	29.079092
338.573739	17023.733054	29.084109
338.926390	17042.735072	29.089127
339.335002	17071.725214	29.094144
339.595332	17092.521985	29.099162
340.179203	17125.117813	29.104180
340.563130	17148.840021	29.109197
340.504140	17179.253618	29.114215
341.261780	17201.733639	29.119232
341.004622	17230.487299	29.124250
341.601448	17264.559682	29.129268
342.114847	17291.104066	29.134285
342.144063	17317.969632	29.139303
342.678339	17342.772160	29.144320
342.850961	17372.280968	29.149338
343.290714	17387.667489	29.154356
343.673692	17421.471328	29.159373
344.104382	17435.888479	29.164391
344.535734	17460.812215	29.169408
344.845485	17474.029431	29.174426
344.920911	17515.591704	29.179444
345.338173	17535.814605	29.184461
345.268112	17556.787909	29.189479
345.765942	17587.600459	29.194496
345.599369	17625.498983	29.199514
346.686825	17656.400244	29.204532
346.801683	17682.653307	29.209549
346.986400	17708.707306	29.214567
347.794831	17736.270745	29.219584
347.947863	17767.499965	29.224602
348.503892	17806.683914	29.229620
348.840613	17825.081058	29.234637
349.429423	17845.928544	29.239655
350.099828	17876.293857	29.244672
350.051261	17894.108486	29.249690
350.313175	17923.559396	29.254708
350.865425	17939.550450	29.259725
351.053238	17972.910071	29.264743
351.559470	17987.821190	29.269760
351.986272	18016.472683	29.274778
351.928896	18054.986214	29.279796
352.268042	18072.276728	29.284813
352.292012	18105.019011	29.289831
352.848200	18137.909868	29.294848
353.336308	18163.988547	29.299866
353.103828	18205.994329	29.304884
353.685660	18242.552202	29.309901
354.283387	18286.999759	29.314919
354.945099	18306.910533	29.319936
354.994198	18337.863243	29.324954
355.146567	18372.025529	29.329972
355.915595	18405.006281	29.334989
356.152027	18428.327534	29.340007
356.900042	18467.099883	29.345024
356.742562	18500.957388	29.350042
357.245580	18530.995325	29.355060
357.564646	18564.982302	29.360077
358.121658	18600.170563	29.365095
358.121058	18620.589927	29.370112
358.686245	18655.863652	29.375130
359.102960	18692.793427	29.380148
359.693216	18715.823344	29.385165
359.902807	18753.285576	29.390183
360.169780	18780.692737	29.395200
360.988194	18808.576309	29.400218
360.808338	18836.850253	29.405236
361.664983	18856.045378	29.410253
361.561264	18887.405823	29.415271
362.177137	18926.142755	29.420288
362.249037	18951.645153	29.425306
363.086978	18990.878342	29.430324
363.726083	19013.766619	29.435341
363.934542	19037.288814	29.440359
364.364438	19068.495243	29.445376
364.500764	19089.415900	29.450394
364.765695	19112.255785	29.455412
364.957788	19133.561364	29.460429
365.244108	19168.752993	29.465447
365.609562	19185.709299	29.470464
366.039673	19225.549521	29.475482
366.714750	19256.933334	29.480500
367.167967	19278.233794	29.485517
366.830862	19314.088318	29.490535
367.461963	19340.014395	29.495552
367.976190	19369.905403	29.500570
368.023818	19394.942741	29.505588
368.186682	19413.543773	29.510605
368.736228	19449.870043	29.515623
369.249836	19468.236642	29.520640
369.885929	19501.479572	29.525658
369.950097	19535.505919	29.530676
370.281197	19559.449973	29.535693
370.614925	19595.720787	29.540711
371.054800	19623.025111	29.545728
371.585326	19665.165482	29.550746
371.950082	19685.119095	29.555764
372.409211	19711.392589	29.560781
372.308150	19749.267800	29.565799
373.314732	19772.851507	29.570816
373.532410	19805.123755	29.575834
373.771699	19828.791735	29.580852
374.379541	19847.956603	29.585869
374.583602	19877.844592	29.590887
374.707440	19913.383070	29.595904
375.574181	19945.048649	29.600922
375.600380	19969.146129	29.605940
376.282226	20006.320357	29.610957
376.172679	20034.989855	29.615975
376.582536	20071.192379	29.620992
376.934642	20108.572643	29.626010
377.200370	20141.586401	29.631028
377.360026	20183.926501	29.636045
377.653957	20221.688664	29.641063
378.179625	20255.876706	29.646080
378.819259	20295.798382	29.651098
379.064514	20329.941467	29.656116
380.108864	20367.665121	29.661133
380.375762	20391.241058	29.666151
380.672426	20417.036469	29.671168
381.446002	20441.873481	29.676186
381.653568	20471.580665	29.681204
382.003195	20505.060523	29.686221
381.967159	20536.488560	29.691239
382.288694	20574.485005	29.696256
382.775037	20609.448004	29.701274
383.288605	20652.722420	29.706292
383.720810	20684.347687	29.711309
384.102354	20717.436465	29.716327
384.259552	20758.077416	29.721344
384.871007	20773.266890	29.726362
385.275754	20813.408327	29.731380
385.858448	20839.887051	29.736397
386.165135	20878.331209	29.741415
386.715128	20905.441303	29.746432
387.023884	20943.629878	29.751450
387.250036	20970.766776	29.756468
388.109157	20999.530146	29.761485
388.165307	21027.333700	29.766503
388.640837	21047.852375	29.771520
388.999371	21080.490064	29.776538
389.415405	21111.860266	29.781556
389.866192	21129.584830	29.786573
390.075272	21160.212092	29.791591
390.405048	21205.572497	29.796608
390.785012	21226.531261	29.801626
391.085883	21260.211446	29.806644
391.912251	21288.911360	29.811661
392.284960	21318.468222	29.816679
392.468291	21365.732472	29.821696
392.876645	21387.169166	29.826714
392.955682	21412.752974	29.831732
393.171278	21439.269644	29.836749
393.499965	21479.415785	29.841767
393.843677	21504.151973	29.846784
394.149532	21535.405588	29.851802
394.463210	21569.197789	29.856820
394.844376	21607.374340	29.861837
395.162490	21650.275299	29.866855
394.955288	21697.389008	29.871872
395.737769	21728.502760	29.876890
396.426987	21771.106239	29.881908
396.834157	21818.973298	29.886925
397.454794	21856.776624	29.891943
397.662684	21895.138534	29.896960
398.216936	21927.846444	29.901978
398.478458	21956.096892	29.906996
398.971419	22003.332283	29.912013
399.376940	22028.126827	29.917031
399.797437	22061.090428	29.922048
400.618965	22109.982449	29.927066
400.928182	22138.401903	29.932084
401.563991	22179.301475	29.937101
402.037332	22204.315261	29.942119
401.638860	22252.786473	29.947136
402.675559	22272.904933	29.952154
402.856782	22307.073662	29.957172
403.272822	22349.362691	29.962189
403.917061	22374.625985	29.967207
403.933030	22410.876567	29.972224
404.714841	22441.312227	29.977242
404.958778	22485.831007	29.982260
405.466956	22523.632339	29.987277
405.773021	22555.721860	29.992295
405.989006	22592.709192	29.997312
406.676495	22622.011387	30.002330
406.704842	22660.453578	30.007348
407.316248	22700.149156	30.012365
407.403996	22745.804390	30.017383
407.692329	22787.019836	30.022400
408.796523	22829.965806	30.027418
408.666546	22869.896199	30.032436
409.049522	22909.700956	30.037453
409.854565	22947.186165	30.042471
409.774163	23000.102089	30.047488
410.543764	23029.093436	30.052506
410.571619	23076.599450	30.057524
411.532040	23116.597841	30.062541
411.954286	23152.237364	30.067559
412.160954	23189.445128	30.072576
412.831168	23218.897850	30.077594
412.908934	23264.652313	30.082612
413.414393	23302.615090	30.087629
414.058137	23349.796239	30.092647
413.887077	23394.564139	30.097664
414.852615	23427.799871	30.102682
415.048962	23474.255875	30.107700
415.650595	23516.175022	30.112717
416.456024	23546.569364	30.117735
416.699026	23581.821569	30.122752
417.487418	23615.172078	30.127770
417.648115	23634.897639	30.132788
418.008780	23671.762523	30.137805
418.591154	23701.145454	30.142823
418.820685	23742.260995	30.147840
419.368415	23769.612603	30.152858
419.596714	23803.803390	30.157876
420.242782	23838.226395	30.162893
420.677356	23864.657100	30.167911
420.607651	23896.563690	30.172928
421.022174	23923.473982	30.177946
421.290684	23963.741627	30.182964
421.743536	23995.103240	30.187981
421.988294	24031.544981	30.192999
422.492827	24067.756250	30.198016
423.235043	24098.515227	30.203034
423.312143	24146.249471	30.208052
423.565264	24191.132310	30.213069
423.883087	24213.136285	30.218087
424.133491	24272.690309	30.223104
424.518351	24309.858484	30.228122
425.020506	24362.958371	30.233140
425.115156	24407.929456	30.238157
426.029877	24443.105604	30.243175
426.310775	24501.876446	30.248192
426.852470	24540.808914	30.253210
427.623600	24573.525551	30.258228
427.686230	24625.117302	30.263245
428.768870	24665.909667	30.268263
428.945444	24704.612687	30.273280
429.459841	24754.696855	30.278298
429.757768	24783.039050	30.283316
430.114572	24818.760696	30.288333
430.756033	24861.829274	30.293351
431.200301	24911.515505	30.298368
431.810542	24954.239411	30.303386
431.784984	24996.169636	30.308404
432.223733	25036.473200	30.313421
433.112427	25075.483607	30.318439
433.344966	25120.872170	30.323456
433.920108	25157.458859	30.328474
434.113870	25199.553619	30.333492
434.289331	25234.995448	30.338509
434.570478	25296.132750	30.343527
434.966664	25335.690296	30.348544
436.018473	25375.773548	30.353562
436.539880	25428.545585	30.358580
436.452234	25474.194554	30.363597
437.259880	25510.024522	30.368615
437.684431	25562.746743	30.373632
438.443049	25595.468993	30.378650
438.646713	25649.117355	30.383668
439.008821	25680.832956	30.388685
439.536545	25721.809409	30.393703
439.748940	25765.589808	30.398720
440.335682	25806.865796	30.403738
440.852320	25860.967745	30.408756
441.042195	25907.847780	30.413773
441.697420	25940.843239	30.418791
442.189578	25988.544041	30.423808
442.915272	26030.403170	30.428826
443.243648	26071.501701	30.433844
443.686011	26119.810343	30.438861
444.145061	26149.716207	30.443879
444.727005	26192.369042	30.448896
445.249788	26233.505237	30.453914
445.879796	26257.715373	30.458932
446.240142	26290.047420	30.463949
446.568325	26331.928796	30.468967
446.871416	26367.689367	30.473984
447.150063	26409.140709	30.479002
447.838618	26444.771534	30.484020
448.000268	26486.611408	30.489037
448.690917	26529.789619	30.494055
448.737853	26574.793216	30.499072
449.190514	26611.841666	30.504090
449.743810	26669.620877	30.509108
450.059370	26708.250282	30.514125
450.314063	26739.783731	30.519143
450.711461	26790.359999	30.524160
451.190177	26833.040944	30.529178
451.647641	26869.060928	30.534196
451.862397	26909.770208	30.539213
452.518397	26958.613662	30.544231
452.826751	27003.849607	30.549248
453.012253	27060.577489	30.554266
453.566831	27109.718842	30.559284
453.970924	27158.960894	30.564301
454.525285	27202.838298	30.569319
455.215255	27256.685770	30.574336
455.511649	27313.175376	30.579354
456.096338	27357.972336	30.584372
456.400792	27407.849777	30.589389
456.897586	27462.991478	30.594407
457.569183	27494.312353	30.599424
457.743371	27553.797343	30.604442
458.654072	27591.668042	30.609460
458.757568	27638.948732	30.614477
459.198397	27691.570722	30.619495
459.432147	27745.422538	30.624512
459.701556	27800.587109	30.629530
460.769602	27848.305198	30.634548
460.963134	27907.917539	30.639565
461.730627	27954.710900	30.644583
462.429910	28014.489256	30.649600
462.515140	28070.896363	30.654618
463.181678	28112.637865	30.659636
463.068750	28170.506932	30.664653
464.007808	28215.203426	30.669671
464.585118	28259.231139	30.674688
464.730404	28323.174326	30.679706
465.809885	28366.734532	30.684724
465.738353	28426.499695	30.689741
466.754864	28469.348212	30.694759
467.160387	28522.076353	30.699776
467.641160	28570.353991	30.704794
468.427223	28614.013761	30.709812
468.550764	28659.246724	30.714829
469.236185	28703.286101	30.719847
469.393370	28749.207715	30.724864
470.195468	28783.619643	30.729882
471.101971	28826.518764	30.734900
470.994903	28877.903698	30.739917
471.766876	28924.061749	30.744935
472.005319	28977.232109	30.749952
472.222890	29005.085106	30.754970
472.988495	29054.821731	30.759988
473.314572	29105.580602	30.765005
473.771747	29146.614726	30.770023
473.990183	29208.511291	30.775040
474.348438	29250.508354	30.780058
474.965828	29300.408965	30.785076
475.622750	29365.757267	30.790093
476.023256	29400.369249	30.795111
476.916711	29455.890270	30.800128
477.261547	29504.792332	30.805146
477.920786	29532.573221	30.810164
478.224151	29589.447660	30.815181
478.861705	29630.415279	30.820199
479.266346	29671.730617	30.825216
479.765484	29725.992707	30.830234
480.158381	29757.111357	30.835252
480.812958	29808.130327	30.840269
481.461999	29847.064985	30.845287
481.666253	29888.237280	30.850304
481.849838	29932.252262	30.855322
482.639745	29970.993580	30.860340
482.980944	30014.067886	30.865357
483.000457	30048.816651	30.870375
483.663307	30089.718081	30.875392
484.093826	30143.352410	30.880410
484.749189	30189.845405	30.885428
485.014077	30239.933129	30.890445
485.502435	30281.762923	30.895463
485.654220	30321.657789	30.900480
485.825181	30395.525933	30.905498
486.785698	30441.824078	30.910516
487.379942	30502.394966	30.915533
487.381969	30546.362619	30.920551
488.290037	30591.997866	30.925568
488.808177	30658.146863	30.930586
489.551507	30698.563214	30.935604
489.782485	30751.412130	30.940621
490.536819	30812.276283	30.945639
491.058456	30854.420588	30.950656
491.313101	30911.726978	30.955674
491.931892	30946.488959	30.960692
492.234436	31010.731531	30.965709
493.206906	31062.013993	30.970727
494.006822	31103.911024	30.975744
493.750185	31161.615016	30.980762
494.759223	31203.897341	30.985780
494.898447	31258.520208	30.990797
495.517888	31306.236742	30.995815
495.803924	31351.187999	31.000832
496.307921	31409.208850	31.005850
497.136277	31447.394992	31.010868
497.620146	31509.202242	31.015885
497.630598	31556.404839	31.020903
498.537200	31621.947512	31.025920
498.588884	31671.790608	31.030938
499.159883	31726.854717	31.035956
499.433517	31780.368544	31.040973
499.877791	31837.706584	31.045991
500.543409	31906.038116	31.051008
500.755092	31964.311007	31.056026
501.862236	32022.799008	31.061044
502.322790	32077.560648	31.066061
502.810874	32137.485863	31.071079
503.293322	32196.673932	31.076096
503.695647	32259.835035	31.081114
504.208354	32310.616566	31.086132
504.405115	32377.588665	31.091149
505.114514	32442.649542	31.096167
506.065969	32497.255682	31.101184
506.656228	32554.057663	31.106202
507.243867	32585.874858	31.111220
507.825332	32646.568853	31.116237
508.417292	32701.922826	31.121255
508.988658	32741.286931	31.126272
509.362347	32795.702312	31.131290
510.014912	32845.474721	31.136308
510.657146	32901.145999	31.141325
510.892958	32953.760951	31.146343
511.339883	33002.974597	31.151360
511.855173	33054.360488	31.156378
512.357098	33105.521561	31.161396
512.729056	33155.691424	31.166413
513.092764	33210.683984	31.171431
514.006048	33260.638522	31.176448
514.490922	33307.565512	31.181466
515.189055	33354.886516	31.186484
515.284250	33400.414078	31.191501
515.830677	33458.403127	31.196519
516.523497	33502.264068	31.201536
516.947993	33561.485223	31.206554
517.440616	33592.685717	31.211572
518.055315	33644.842576	31.216589
518.093340	33684.514596	31.221607
518.830297	33739.115840	31.226624
519.057733	33797.243883	31.231642
519.776360	33840.104314	31.236660
520.339214	33898.347674	31.241677
520.366007	33947.040138	31.246695
521.255738	33985.704427	31.251712
521.577735	34060.405493	31.256730
522.438095	34112.381160	31.261748
522.876439	34165.206071	31.266765
522.912475	34222.616136	31.271783
523.933531	34273.691686	31.276800
524.277268	34330.022607	31.281818
524.709131	34396.035820	31.286836
525.394289	34461.644563	31.291853
525.604347	34512.517123	31.296871
526.452383	34565.278709	31.301888
526.752788	34638.310216	31.306906
527.222879	34677.294613	31.311924
528.084601	34754.935566	31.316941
528.275409	34816.578761	31.321959
528.931356	34865.668392	31.326976
529.265799	34938.338934	31.331994
530.155981	35003.758036	31.337012
530.434378	35059.423617	31.342029
530.497913	35127.977497	31.347047
531.571472	35187.103178	31.352064
532.175416	35250.200623	31.357082
532.801140	35313.424075	31.362100
533.374842	35375.305740	31.367117
533.869539	35442.325406	31.372135
534.630777	35494.652832	31.377152
535.082228	35568.477356	31.382170
535.772434	35629.867313	31.387188
536.285826	35686.174502	31.392205
536.730788	35748.075568	31.397223
537.569884	35795.591228	31.402240
537.683737	35860.400116	31.407258
538.307879	35919.813892	31.412276
539.080736	35976.173809	31.417293
539.665379	36037.996006	31.422311
539.897857	36104.215729	31.427328
540.224853	36168.046958	31.432346
540.829094	36221.304991	31.437364
541.857282	36291.673196	31.442381
541.921556	36350.956817	31.447399
542.427263	36409.978374	31.452416
542.952512	36474.598456	31.457434
543.408633	36547.785619	31.462452
544.081407	36609.080830	31.467469
544.613937	36676.600648	31.472487
545.174984	36735.159693	31.477504
545.457935	36808.774160	31.482522
545.942658	36877.363000	31.487540
546.422334	36947.041718	31.492557
546.761025	37028.540763	31.497575
547.553514	37094.425481	31.502592
548.239229	37166.226508	31.507610
548.689218	37239.928763	31.512628
549.622494	37301.833436	31.517645
549.967628	37380.464249	31.522663
550.795376	37434.238103	31.527680
551.205742	37500.774437	31.532698
551.643451	37569.730309	31.537716
552.462903	37618.005175	31.542733
552.906860	37687.743156	31.547751
553.733809	37737.311073	31.552768
554.316176	37799.625738	31.557786
554.820865	37851.929832	31.562804
555.494581	37895.230332	31.567821
555.572107	37960.374706	31.572839
556.116866	38010.226688	31.577856
556.715887	38086.050763	31.582874
557.225460	38135.448113	31.587892
557.815092	38191.576979	31.592909
558.352961	38267.244641	31.597927
558.916663	38324.899455	31.602944
559.374594	38391.737361	31.607962
559.607972	38465.126909	31.612980
560.437512	38534.028057	31.617997
560.990667	38606.715191	31.623015
561.426102	38660.276599	31.628032
561.654563	38745.762622	31.633050
562.293092	38820.816293	31.638068
563.125463	38886.729376	31.643085
563.329763	38973.138924	31.648103
564.274332	39035.991399	31.653120
565.012948	39109.536826	31.658138
565.437202	39177.655169	31.663156
566.174581	39239.160119	31.668173
566.843988	39316.110827	31.673191
567.582949	39382.110579	31.678208
567.895954	39448.988944	31.683226
568.525271	39520.754982	31.688244
569.388000	39587.296866	31.693261
569.902898	39661.661098	31.698279
570.246474	39723.999729	31.703296
571.357811	39791.438742	31.708314
571.444814	39859.526963	31.713332
572.455296	39914.455348	31.718349
572.515021	39987.062215	31.723367
573.344644	40056.423653	31.728384
573.768199	40125.637787	31.733402
574.507159	40193.130323	31.738420
575.328873	40258.485138	31.743437
575.875815	40330.103835	31.748455
576.506189	40392.634120	31.753472
576.681733	40460.062876	31.758490
577.295168	40520.254271	31.763508
578.188144	40581.536043	31.768525
578.600299	40644.355754	31.773543
579.007952	40717.839236	31.778560
579.721456	40782.803450	31.783578
580.082330	40851.781319	31.788596
581.100488	40922.213396	31.793613
581.774200	40998.504456	31.798631
582.320618	41067.111579	31.803648
582.972647	41122.162782	31.808666
583.957951	41188.939638	31.813684
584.297157	41238.263073	31.818701
584.566427	41315.758643	31.823719
585.138522	41380.530526	31.828736
585.763247	41440.154884	31.833754
586.095953	41512.937369	31.838772
587.145307	41582.101003	31.843789
587.276342	41648.319841	31.848807
587.658364	41718.257115	31.853824
588.486585	41786.343720	31.858842
588.458368	41857.915020	31.863860
589.215712	41933.675293	31.868877
589.590445	42011.143749	31.873895
590.385353	42084.900206	31.878912
590.780878	42150.237462	31.883930
591.366224	42233.865697	31.888948
591.975761	42302.293385	31.893965
592.565589	42373.695159	31.898983
593.054056	42453.972056	31.904000
593.888214	42519.509664	31.909018
594.325350	42589.046535	31.914036
595.193812	42661.846094	31.919053
595.949114	42726.983912	31.924071
596.336689	42804.229440	31.929088
596.901682	42882.550909	31.934106
597.207871	42954.892030	31.939124
598.293387	43021.084430	31.944141
598.961408	43090.105199	31.949159
599.033293	43179.852307	31.954176
600.081419	43243.646070	31.959194
600.655485	43313.844960	31.964212
601.490042	43379.480265	31.969229
602.077559	43451.398023	31.974247
602.481165	43539.276800	31.979264
603.392165	43600.682473	31.984282
603.788120	43680.629543	31.989300
604.560411	43747.624500	31.994317
604.721969	43830.698540	31.999335
605.707095	43902.116699	32.004352
606.420111	43959.843522	32.009370
607.031413	44034.493662	32.014388
607.707094	44097.089035	32.019405
608.082805	44177.309943	32.024423
608.540766	44259.061459	32.029440
609.420080	44325.305209	32.034458
609.704035	44421.129244	32.039476
610.409039	44484.939752	32.044493
610.808310	44559.251312	32.049511
611.187189	44638.207644	32.054528
612.378243	44726.505020	32.059546
612.450136	44799.286677	32.064564
613.266491	44889.875727	32.069581
614.148254	44967.339102	32.074599
614.497146	45039.712860	32.079616
615.366383	45127.200191	32.084634
615.954032	45203.162887	32.089652
616.640722	45285.319993	32.094669
617.025544	45367.461012	32.099687
617.868330	45455.023708	32.104704
618.325599	45526.822602	32.109722
618.866259	45615.563128	32.114740
619.452177	45702.013803	32.119757
620.480734	45781.735951	32.124775
620.544156	45862.877650	32.129792
621.466060	45947.947852	32.134810
621.950965	46026.403132	32.139828
622.342169	46105.941438	32.144845
623.165203	46185.850808	32.149863
623.594445	46281.088873	32.154880
624.074513	46364.001586	32.159898
624.595930	46459.834732	32.164916
625.412287	46544.116742	32.169933
626.304306	46632.084127	32.174951
626.912228	46717.102315	32.179968
627.941643	46794.798312	32.184986
628.869580	46883.765053	32.190004
629.538260	46963.198007	32.195021
629.819877	47037.172543	32.200039
630.524012	47120.853620	32.205056
631.070715	47188.656003	32.210074
631.584228	47267.203305	32.215092
632.311095	47342.232786	32.220109
633.017893	47408.926439	32.225127
633.582772	47480.746600	32.230144
634.678480	47552.694088	32.235162
634.913838	47622.159880	32.240180
635.458382	47689.414975	32.245197
636.078888	47765.669958	32.250215
636.645300	47833.262990	32.255232
637.658815	47914.013459	32.260250
637.730090	47990.641098	32.265268
638.406918	48071.558367	32.270285
638.993195	48145.733233	32.275303
639.402996	48229.028894	32.280320
640.400354	48303.063854	32.285338
641.090752	48393.062180	32.290356
641.399781	48472.933503	32.295373
642.113968	48546.908815	32.300391
642.399972	48645.018225	32.305408
643.555830	48733.845507	32.310426
643.792044	48815.808197	32.315444
644.287148	48899.256920	32.320461
645.586759	48977.179375	32.325479
645.885359	49072.067805	32.330496
646.163893	49151.403844	32.335514
646.987809	49252.108663	32.340532
647.424520	49355.514898	32.345549
648.547971	49438.416932	32.350567
649.104064	49535.488388	32.355584
649.962100	49607.419767	32.360602
650.507255	49694.969172	32.365620
651.608690	49804.378908	32.370637
652.144342	49862.620533	32.375655
652.742792	49960.868282	32.380672
653.842942	50039.099622	32.385690
654.597089	50127.560772	32.390708
655.372060	50201.131387	32.395725
656.006019	50274.261326	32.400743
656.572315	50355.433945	32.405760
656.906590	50442.585773	32.410778
657.538217	50528.065574	32.415796
657.839317	50608.316653	32.420813
658.526443	50698.108481	32.425831
658.944469	50806.338782	32.430848
659.609556	50885.975057	32.435866
660.131761	50981.287658	32.440884
661.055864	51074.118267	32.445901
661.919607	51161.684925	32.450919
662.389860	51261.741794	32.455936
663.304272	51341.569338	32.460954
663.698162	51445.395031	32.465972
664.161234	51531.677771	32.470989
665.126504	51620.142516	32.476007
666.005650	51724.123290	32.481024
666.618283	51804.169987	32.486042
667.269837	51914.771501	32.491060
667.662980	51996.203891	32.496077
668.706898	52091.413715	32.501095
668.873550	52176.987106	32.506112
670.241597	52266.196865	32.511130
670.766186	52368.205600	32.516148
671.419001	52456.744734	32.521165
672.183688	52536.737769	32.526183
672.537825	52630.525963	32.531200
673.238737	52728.041294	32.536218
674.264994	52813.393412	32.541236
674.719672	52894.828896	32.546253
675.577648	52989.009403	32.551271
676.245205	53085.995081	32.556288
676.942232	53162.836941	32.561306
677.356229	53245.544067	32.566324
677.898272	53333.480088	32.571341
678.567186	53414.970815	32.576359
679.038841	53508.661717	32.581376
679.561377	53589.166569	32.586394
680.190312	53687.039742	32.591412
680.858315	53769.125941	32.596429
681.745475	53870.874217	32.601447
682.098606	53967.505580	32.606464
682.686464	54058.924582	32.611482
683.437284	54160.494723	32.616500
683.884414	54252.929735	32.621517
684.923511	54354.491184	32.626535
685.287594	54457.124925	32.631552
686.036868	54549.846280	32.636570
686.653510	54653.254325	32.641588
687.433628	54765.720883	32.646605
688.854935	54867.379821	32.651623
689.266721	54970.627521	32.656640
689.663041	55078.250292	32.661658
690.560646	55167.614237	32.666676
690.845708	55269.551360	32.671693
691.801740	55374.511919	32.676711
692.258907	55472.441349	32.681728
693.077486	55584.021727	32.686746
694.013819	55685.373280	32.691764
694.445249	55792.678262	32.696781
695.259341	55907.710905	32.701799
695.828735	56006.843863	32.706816
696.614820	56110.023097	32.711834
697.292016	56223.942917	32.716852
698.325209	56326.741292	32.721869
698.803792	56422.207778	32.726887
699.462567	56532.979588	32.731904
700.613430	56643.961398	32.736922
701.219281	56741.228102	32.741940
702.022224	56844.376799	32.746957
702.578931	56952.520387	32.751975
703.412854	57046.705422	32.756992
704.004544	57152.790810	32.762010
704.945950	57266.262299	32.767028
705.443847	57366.778698	32.772045
706.054604	57472.180237	32.777063
706.857428	57583.237428	32.782080
707.494683	57675.890898	32.787098
708.476912	57786.331957	32.792116
708.837694	57891.498978	32.797133
710.068374	58003.397764	32.802151
710.675599	58110.174452	32.807168
711.340861	58200.626783	32.812186
712.205156	58315.665124	32.817204
712.815250	58415.707016	32.822221
713.646732	58510.152151	32.827239
714.325212	58619.042974	32.832256
715.559695	58703.779668	32.837274
715.869288	58794.742081	32.842292
716.612943	58904.539962	32.847309
717.523000	58997.066057	32.852327
718.468382	59100.316680	32.857344
718.861817	59193.535640	32.862362
719.798230	59292.605432	32.867380
720.655403	59388.712433	32.872397
721.118224	59476.455099	32.877415
721.808035	59566.467210	32.882432
722.286922	59670.082177	32.887450
722.939629	59757.207014	32.892468
723.063453	59867.093572	32.897485
723.890750	59974.532686	32.902503
724.600996	60077.498561	32.907520
725.003488	60176.566100	32.912538
726.095320	60280.038752	32.917556
726.524190	60371.026530	32.922573
727.651225	60485.098649	32.927591
728.152821	60584.455167	32.932608
728.904888	60685.767825	32.937626
729.762447	60780.086633	32.942644
730.302825	60903.522665	32.947661
731.220031	61008.411916	32.952679
731.636725	61107.298407	32.957696
732.389251	61222.359230	32.962714
733.279250	61314.981466	32.967732
733.660796	61430.281691	32.972749
734.333391	61537.495562	32.977767
735.229360	61664.347152	32.982784
735.663320	61774.420388	32.987802
736.482988	61877.984093	32.992820
737.185503	62004.692797	32.997837
738.057101	62126.198200	33.002855
738.951768	62255.537503	33.007872
739.538551	62365.753029	33.012890
740.309276	62479.098884	33.017908
740.776899	62610.931610	33.022925
741.676845	62718.999007	33.027943
742.439807	62844.122882	33.032960
742.843816	62969.009744	33.037978
744.126155	63086.370089	33.042996
744.617647	63216.344584	33.048013
745.442005	63331.304352	33.053031
746.317433	63450.927195	33.058048
746.845777	63578.432902	33.063066
747.551699	63698.533944	33.068084
748.119602	63836.128713	33.073101
749.054993	63970.674039	33.078119
749.753931	64093.041346	33.083136
750.206197	64233.932009	33.088154
751.145072	64355.205688	33.093172
751.869451	64487.911971	33.098189
752.689464	64628.264222	33.103207
753.751150	64745.190118	33.108224
754.718201	64876.202749	33.113242
755.221860	65002.223298	33.118260
755.870376	65133.574611	33.123277
756.769862	65259.784208	33.128295
757.783602	65401.487723	33.133312
758.585687	65518.258595	33.138330
759.520325	65634.496220	33.143348
759.955676	65759.243142	33.148365
760.914612	65896.205534	33.153383
761.553762	66015.186952	33.158400
762.459591	66139.529761	33.163418
763.236275	66270.791267	33.168436
764.177816	66381.740948	33.173453
764.749537	66506.924985	33.178471
765.610038	66641.487434	33.183488
766.326047	66753.013666	33.188506
767.063236	66878.766839	33.193524
767.846166	67012.939917	33.198541
768.810210	67123.491576	33.203559
769.681165	67247.378964	33.208576
770.255575	67375.412529	33.213594
770.952697	67499.405979	33.218612
771.535734	67632.484454	33.223629
772.217527	67743.016462	33.228647
773.311929	67874.362034	33.233664
774.063834	67997.262026	33.238682
775.541818	68116.824971	33.243700
776.147562	68220.816208	33.248717
776.861663	68326.819429	33.253735
777.698720	68443.164700	33.258752
778.334608	68541.721919	33.263770
779.239253	68645.577392	33.268788
779.995364	68764.074676	33.273805
780.581896	68871.081640	33.278823
781.492779	68975.923972	33.283840
781.951543	69084.053179	33.288858
782.914266	69197.865624	33.293876
783.579161	69312.284228	33.298893
784.547881	69428.404567	33.303911
785.472955	69533.898531	33.308928
786.262954	69655.107523	33.313946
787.143358	69756.500415	33.318964
787.702187	69881.965942	33.323981
788.368043	69996.242672	33.328999
789.533941	70094.605819	33.334016
790.264518	70218.053379	33.339034
790.956785	70332.719562	33.344052
791.696242	70450.097306	33.349069
792.478580	70565.173488	33.354087
793.353819	70694.802474	33.359104
793.718285	70805.308090	33.364122
794.535485	70927.202717	33.369140
795.112036	71062.883586	33.374157
796.016821	71180.465682	33.379175
796.802938	71314.374762	33.384192
797.186471	71440.080764	33.389210
798.138626	71570.214533	33.394228
798.941634	71710.604354	33.399245
799.280068	71839.740903	33.404263
800.584368	71976.161014	33.409280
801.356447	72117.273120	33.414298
802.260766	72253.248871	33.419316
803.112914	72376.119762	33.424333
803.689148	72528.604430	33.429351
804.735721	72650.142194	33.434368
805.421638	72788.800537	33.439386
806.338754	72929.868741	33.444404
807.134720	73060.562187	33.449421
807.769867	73200.666981	33.454439
808.956658	73335.641771	33.459456
809.708941	73479.327099	33.464474
810.679924	73606.782602	33.469492
811.700386	73733.332735	33.474509
812.140940	73868.965267	33.479527
813.675019	73989.209620	33.484544
814.161724	74131.305302	33.489562
814.848439	74257.040936	33.494580
815.619378	74381.884384	33.499597
816.474594	74523.466470	33.504615
817.495067	74653.025799	33.509632
818.103472	74778.979752	33.514650
819.020187	74901.380057	33.519668
820.136185	75047.172186	33.524685
820.409386	75173.360844	33.529703
821.598237	75305.444838	33.534720
822.183879	75442.992077	33.539738
823.033768	75571.623778	33.544756
823.898138	75702.448335	33.549773
824.732237	75831.615406	33.554791
825.711238	75961.739571	33.559808
826.240874	76110.671271	33.564826
826.925475	76235.451052	33.569844
827.830394	76368.593926	33.574861
828.319639	76515.574490	33.579879
829.261207	76638.891141	33.584896
830.004028	76783.206978	33.589914
831.120376	76919.297115	33.594932
831.939404	77032.567562	33.599949
832.712725	77155.301410	33.604967
833.746726	77273.350617	33.609984
834.428767	77413.285003	33.615002
835.079759	77537.426281	33.620020
836.038685	77672.901948	33.625037
836.352230	77799.737839	33.630055
837.973517	77934.346765	33.635072
838.468949	78080.185621	33.640090
839.094851	78214.233252	33.645108
840.140661	78345.960679	33.650125
840.979801	78482.460422	33.655143
841.970709	78618.354043	33.660160
842.924962	78757.771278	33.665178
843.419069	78894.102821	33.670196
844.330785	79030.087937	33.675213
844.729370	79172.477459	33.680231
845.958275	79315.192527	33.685248
846.707883	79458.816260	33.690266
847.375218	79599.804204	33.695284
848.217356	79751.947365	33.700301
849.017045	79897.950304	33.705319
849.661875	80046.358123	33.710336
850.801389	80189.979100	33.715354
851.212033	80352.046332	33.720372
852.236644	80506.403718	33.725389
853.055889	80670.670329	33.730407
854.403837	80813.735859	33.735424
854.996916	80965.637401	33.740442
855.643853	81131.017516	33.745460
856.722635	81287.281688	33.750477
857.629460	81445.795696	33.755495
858.628708	81597.685037	33.760512
859.144245	81745.967272	33.765530
860.167295	81906.622454	33.770548
861.256188	82060.524404	33.775565
861.727816	82218.831022	33.780583
862.866546	82377.490396	33.785600
863.806571	82529.054158	33.790618
864.701675	82696.416443	33.795636
865.588037	82843.600808	33.800653
866.247781	83016.349951	33.805671
867.337545	83164.913563	33.810688
868.189695	83319.622290	33.815706
868.951009	83484.734979	33.820724
870.172759	83626.890163	33.825741
870.918993	83802.439907	33.830759
871.625620	83949.332107	33.835776
872.836848	84102.892361	33.840794
873.220160	84259.336089	33.845812
874.363969	84411.479732	33.850829
875.033047	84585.624720	33.855847
875.956559	84740.761481	33.860864
877.177262	84900.544680	33.865882
877.704824	85056.052629	33.870900
879.005426	85205.606952	33.875917
879.766836	85380.444987	33.880935
880.581999	85522.995392	33.885952
881.608787	85683.189324	33.890970
882.273196	85843.134176	33.895988
883.486527	85997.010414	33.901005
884.258044	86154.326650	33.906023
885.387348	86304.681949	33.911040
886.211767	86462.042154	33.916058
887.028499	86608.123226	33.921076
887.977628	86745.489679	33.926093
888.635795	86901.228888	33.931111
889.608482	87033.948904	33.936128
890.651217	87182.103271	33.941146
891.214819	87330.154195	33.946164
892.427809	87461.482896	33.951181
893.158247	87620.252156	33.956199
894.164112	87757.033068	33.961216
894.920764	87917.154110	33.966234
895.462175	88060.524575	33.971252
896.566444	88209.409296	33.976269
897.271823	88366.086960	33.981287
897.826014	88521.379542	33.986304
898.799892	88680.292959	33.991322
899.445069	88832.617491	33.996340
900.662279	88998.390222	34.001357
901.349589	89167.801579	34.006375
902.375275	89331.893408	34.011392
903.524446	89500.072871	34.016410
904.209719	89663.368926	34.021428
905.142256	89830.536049	34.026445
905.968025	89993.001180	34.031463
906.886566	90164.469781	34.036480
908.154661	90326.535096	34.041498
909.050262	90504.395131	34.046516
909.828769	90656.785322	34.051533
910.964764	90825.210501	34.056551
912.020239	90987.334409	34.061568
912.552561	91166.873114	34.066586
912.905713	91334.070520	34.071604
914.163718	91503.163816	34.076621
914.754306	91676.716248	34.081639
915.794692	91857.334377	34.086656
916.711229	92044.689056	34.091674
917.773574	92214.914541	34.096692
918.942413	92399.433028	34.101709
919.567528	92577.486033	34.106727
920.393746	92747.418843	34.111744
921.643824	92928.700243	34.116762
922.606104	93119.948024	34.121780
923.738797	93280.213944	34.126797
924.281618	93466.616077	34.131815
925.212156	93648.879679	34.136832
926.166857	93820.127926	34.141850
927.193263	94009.061995	34.146868
928.435726	94179.594370	34.151885
929.343966	94367.614006	34.156903
929.981327	94544.749037	34.161920
931.090432	94704.749763	34.166938
932.162774	94903.702608	34.171956
933.266258	95078.340375	34.176973
934.284374	95257.455802	34.181991
935.337709	95421.958068	34.187008
936.302510	95589.476293	34.192026
937.096424	95770.645304	34.197044
938.214145	95941.014346	34.202061
939.236408	96118.470661	34.207079
940.022161	96276.579144	34.212096
941.052259	96448.922075	34.217114
941.741840	96623.139106	34.222132
942.814266	96800.750296	34.227149
943.990699	96973.990569	34.232167
944.936956	97147.073829	34.237184
945.907254	97325.851382	34.242202
946.669274	97487.168205	34.247220
947.803967	97659.527618	34.252237
948.489908	97840.033309	34.257255
949.660864	98001.026412	34.262272
950.665317	98171.821990	34.267290
951.116018	98345.318255	34.272308
952.027408	98485.872440	34.277325
953.227165	98660.304390	34.282343
953.901289	98825.708506	34.287360
954.673550	98991.629271	34.292378
955.518487	99164.236830	34.297396
956.396743	99341.961507	34.302413
957.254549	99516.664783	34.307431
957.966254	99694.387796	34.312448
958.761280	99862.108458	34.317466
960.028013	100055.556479	34.322484
960.701787	100242.640138	34.327501
961.497597	100424.520074	34.332519
962.277568	100625.269984	34.337536
963.888972	100819.983775	34.342554
964.694090	101000.783721	34.347572
965.349384	101191.676031	34.352589
966.436555	101386.202154	34.357607
967.550287	101576.116315	34.362624
968.394526	101769.957398	34.367642
969.369098	101970.742784	34.372660
970.383913	102162.070509	34.377677
971.437518	102355.286327	34.382695
972.814023	102567.102513	34.387712
973.924259	102741.931924	34.392730
974.581441	102927.303231	34.397748
975.942123	103116.447274	34.402765
976.958828	103313.165057	34.407783
977.947421	103507.799552	34.412800
979.218840	103694.803502	34.417818
980.005411	103882.097801	34.422836
981.120897	104067.749885	34.427853
982.253864	104255.730512	34.432871
983.127656	104433.732000	34.437888
983.995189	104634.866094	34.442906
984.882466	104833.851960	34.447924
985.886123	105017.300460	34.452941
986.744255	105215.534218	34.457959
987.548492	105420.256088	34.462976
988.117028	105620.332707	34.467994
989.067501	105824.704329	34.473012
990.293335	106029.336032	34.478029
991.452260	106234.904889	34.483047
992.030279	106437.569744	34.488064
993.487300	106631.276385	34.493082
994.364827	106844.166019	34.498100
995.283215	107055.252204	34.503117
996.705738	107254.339053	34.508135
997.318921	107459.045019	34.513152
998.737481	107667.938443	34.518170
1000.173919	107862.442759	34.523188
1001.247233	108059.110910	34.528205
1002.052790	108249.605959	34.533223
1003.000295	108454.606375	34.538240
1004.506300	108646.077861	34.543258
1005.368331	108845.560488	34.548276
1006.266183	109033.626736	34.553293
1007.100579	109236.321306	34.558311
1008.208650	109424.380925	34.563328
1009.293662	109623.237228	34.568346
1010.286638	109822.971503	34.573364
1011.368738	110015.029413	34.578381
1012.280461	110211.588070	34.583399
1013.307785	110401.200489	34.588416
1014.279676	110584.857421	34.593434
1015.628049	110788.720156	34.598452
1016.485712	110977.110621	34.603469
1017.423855	111162.499727	34.608487
1018.420873	111362.054711	34.613504
1019.302985	111536.701370	34.618522
1020.119007	111721.772442	34.623540
1020.988932	111903.985748	34.628557
1022.184581	112088.958638	34.633575
1022.898195	112297.206362	34.638592
1024.062290	112483.707221	34.643610
1024.765694	112682.078921	34.648628
1026.000980	112869.964090	34.653645
1027.342288	113073.781746	34.658663
1027.698246	113264.842381	34.663680
1029.136394	113452.774051	34.668698
1030.104838	113673.037343	34.673716
1030.902969	113867.576203	34.678733
1032.186234	114077.706922	34.683751
1032.798377	114274.610301	34.688768
1033.789511	114481.561894	34.693786
1035.088794	114686.323180	34.698804
1036.059632	114894.915438	34.703821
1037.237232	115098.356976	34.708839
1038.114568	115318.623034	34.713856
1039.437860	115511.946516	34.718874
1040.395645	115723.587653	34.723892
1041.385023	115937.454929	34.728909
1042.943867	116156.854931	34.733927
1043.853687	116371.220075	34.738944
1044.600195	116566.964527	34.743962
1045.708906	116784.834732	34.748980
1046.538876	117005.273877	34.753997
1047.822344	117217.556642	34.759015
1048.309267	117441.844043	34.764032
1049.728474	117648.026152	34.769050
1051.081759	117877.698020	34.774068
1051.704406	118099.434221	34.779085
1052.699783	118319.184755	34.784103
1053.819705	118544.326608	34.789120
1054.238657	118770.979693	34.794138
1055.525179	118994.716523	34.799156
1056.337574	119241.074249	34.804173
1057.581277	119465.341311	34.809191
1058.150550	119703.380517	34.814208
1059.539920	119943.681091	34.819226
1060.841837	120188.154176	34.824244
1061.725630	120425.197089	34.829261
1063.113908	120649.386131	34.834279
1063.929579	120899.520804	34.839296
1065.064402	121141.317865	34.844314
1066.214610	121369.049061	34.849332
1067.248982	121622.993300	34.854349
1068.904917	121854.256195	34.859367
1069.898461	122087.809817	34.864384
1070.933865	122320.484029	34.869402
1072.499442	122547.509562	34.874420
1073.398364	122780.450716	34.879437
1074.626466	122998.880416	34.884455
1075.491616	123235.328257	34.889472
1076.272334	123464.201176	34.894490
1077.754839	123701.577291	34.899508
1078.648117	123928.432963	34.904525
1079.571673	124164.092872	34.909543
1080.713139	124399.629964	34.914560
1081.646644	124632.681348	34.919578
1082.781950	124867.703564	34.924596
1083.733436	125111.185564	34.929613
1084.828065	125349.500603	34.934631
1085.732882	125580.941935	34.939648
1086.935696	125826.530027	34.944666
1088.033396	126053.406083	34.949684
1088.997104	126293.359736	34.954701
1090.112299	126511.897140	34.959719
1091.570357	126745.588026	34.964736
1092.443707	126973.712024	34.969754
1093.570320	127200.363770	34.974772
1094.627800	127430.932220	34.979789
1095.481875	127647.987340	34.984807
1096.569571	127884.663162	34.989824
1097.825415	128116.686927	34.994842
1099.117248	128348.795228	34.999860
1100.093578	128580.260269	35.004877
1101.403170	128810.303178	35.009895
1102.458003	129049.870542	35.014912
1103.297359	129276.052716	35.019930
1104.230690	129518.356177	35.024948
1105.361518	129755.787079	35.029965
1106.786538	129991.193917	35.034983
1107.780598	130245.179465	35.040000
1108.989109	130481.462316	35.045018
1109.960876	130723.882899	35.050036
1111.279373	130961.608894	35.055053
1112.256939	131200.888692	35.060071
1113.455474	131453.709496	35.065088
1114.201417	131682.054049	35.070106
1115.908486	131931.169467	35.075124
1116.675862	132183.750404	35.080141
1117.657430	132432.203624	35.085159
1118.925696	132690.017191	35.090176
1120.108002	132934.511590	35.095194
1121.640854	133183.183911	35.100212
1122.043947	133435.682818	35.105229
1123.335909	133685.919998	35.110247
1124.610964	133949.586531	35.115264
1124.949035	134206.906712	35.120282
1126.475376	134468.495061	35.125300
1127.282263	134725.551843	35.130317
1128.484013	134989.923556	35.135335
1130.268298	135256.736706	35.140352
1131.271308	135517.101504	35.145370
1132.755370	135779.087750	35.150388
1133.600646	136042.043623	35.155405
1134.706702	136298.822606	35.160423
1136.228625	136555.458890	35.165440
1137.250062	136818.810293	35.170458
1138.540987	137081.193835	35.175476
1139.340823	137337.080652	35.180493
1140.603909	137600.956256	35.185511
1141.842729	137856.799992	35.190528
1143.165542	138126.108875	35.195546
1144.480784	138372.371858	35.200564
1145.119833	138643.357247	35.205581
1146.530015	138904.100021	35.210599
1147.790960	139172.121682	35.215616
1148.776998	139426.434370	35.220634
1150.226301	139680.888055	35.225652
1151.271467	139943.867265	35.230669
1152.299964	140201.031576	35.235687
1153.376751	140459.014022	35.240704
1154.379302	140722.906555	35.245722
1156.083597	140980.485086	35.250740
1157.217970	141236.080213	35.255757
1158.357660	141501.946836	35.260775
1159.914701	141764.957108	35.265792
1160.646831	142019.369211	35.270810
1162.184656	142270.087165	35.275828
1163.174444	142526.184953	35.280845
1163.807728	142780.187885	35.285863
1165.270831	143046.659769	35.290880
1166.355966	143283.714547	35.295898
1168.184189	143517.845936	35.300916
1169.096291	143769.299397	35.305933
1170.836719	143986.291847	35.310951
1171.993723	144216.214690	35.315968
1172.841376	144456.271231	35.320986
1173.995666	144687.681258	35.326004
1175.256588	144920.127718	35.331021
1175.927615	145171.098455	35.336039
1177.291885	145405.877034	35.341056
1178.492531	145654.988451	35.346074
1179.500209	145901.432384	35.351092
1180.349249	146146.851670	35.356109
1181.275757	146403.356048	35.361127
1182.798355	146654.665937	35.366144
1184.033860	146914.737202	35.371162
1184.861185	147173.901249	35.376180
1186.069592	147447.423384	35.381197
1187.267102	147703.892352	35.386215
1188.348301	147961.954901	35.391232
1189.308850	148223.843809	35.396250
1190.615382	148493.920861	35.401268
1191.638485	148771.681386	35.406285
1192.709588	149048.066421	35.411303
1193.700957	149329.425524	35.416320
1194.517078	149612.489807	35.421338
1195.900851	149900.662433	35.426356
1197.030949	150183.641246	35.431373
1198.376845	150479.269389	35.436391
1199.545889	150777.465667	35.441408
1200.426987	151072.566494	35.446426
1201.738136	151355.575117	35.451444
1202.663674	151664.472497	35.456461
1203.603505	151972.494924	35.461479
1205.039251	152279.157003	35.466496
1205.811953	152593.972368	35.471514
1207.214212	152894.886686	35.476532
1208.443082	153206.042402	35.481549
1209.831483	153512.849162	35.486567
1211.182328	153829.012641	35.491584
1212.529803	154146.447701	35.496602
1213.824511	154446.910070	35.501620
1215.072161	154763.250519	35.506637
1216.323798	155070.472884	35.511655
1217.998039	155377.564519	35.516672
1219.226618	155682.360149	35.521690
1220.664975	155984.954477	35.526708
1222.202634	156279.619504	35.531725
1223.249087	156581.192267	35.536743
1224.743786	156887.475578	35.541760
1225.937542	157173.971598	35.546778
1227.208367	157482.085082	35.551796
1228.688036	157771.671476	35.556813
1229.752426	158068.724061	35.561831
1231.389398	158361.206416	35.566848
1232.164054	158659.046987	35.571866
1233.586062	158946.114358	35.576884
1234.787551	159251.106977	35.581901
1235.778937	159550.199653	35.586919
1237.133567	159847.801091	35.591936
1238.472904	160130.983323	35.596954
1240.092529	160427.403551	35.601972
1241.130957	160722.945041	35.606989
1242.012383	161014.607231	35.612007
1243.900478	161298.265204	35.617024
1245.069133	161607.175649	35.622042
1246.368038	161901.185655	35.627060
1247.241795	162178.483582	35.632077
1248.430638	162464.688146	35.637095
1249.538287	162745.782637	35.642112
1250.672753	163022.104351	35.647130
1251.833036	163300.352045	35.652148
1253.162360	163582.367103	35.657165
1254.275655	163878.515075	35.662183
1255.476653	164157.446834	35.667200
1256.322208	164461.293461	35.672218
1257.531187	164745.201191	35.677236
1258.971165	165042.610192	35.682253
1260.189722	165347.403899	35.687271
1261.366666	165642.728991	35.692288
1262.817495	165952.170399	35.697306
1264.003842	166248.272054	35.702324
1265.473043	166552.906067	35.707341
1266.278653	166855.405980	35.712359
1267.960111	167160.224922	35.717376
1269.147914	167476.051980	35.722394
1270.347219	167776.919976	35.727412
1271.636066	168096.300226	35.732429
1272.932784	168416.595061	35.737447
1274.263328	168718.653232	35.742464
1275.184279	169037.986815	35.747482
1276.264457	169351.396164	35.752500
1277.809443	169666.799269	35.757517
1278.765770	170011.067446	35.762535
1280.180917	170318.261475	35.767552
1281.541502	170654.372283	35.772570
1282.807984	170975.286819	35.777588
1284.174536	171301.110531	35.782605
1285.315895	171635.919721	35.787623
1286.821474	171962.994140	35.792640
1287.548032	172295.326030	35.797658
1289.019130	172623.273718	35.802676
1290.366189	172967.474330	35.807693
1291.474866	173308.354040	35.812711
1293.213185	173645.617218	35.817728
1294.629863	173996.260392	35.822746
1295.886991	174315.499202	35.827764
1297.361407	174650.173609	35.832781
1298.599366	174990.054337	35.837799
1300.095254	175312.699514	35.842816
1301.625146	175654.516489	35.847834
1303.133451	175990.755636	35.852852
1304.479245	176307.099711	35.857869
1305.952073	176634.351568	35.862887
1307.117556	176964.131058	35.867904
1308.470894	177285.988065	35.872922
1309.845559	177615.991252	35.877940
1311.191732	177946.775512	35.882957
1313.215902	178269.023196	35.887975
1314.507282	178579.400752	35.892992
1315.777774	178904.239047	35.898010
1316.939731	179223.411646	35.903028
1318.379352	179532.755361	35.908045
1319.900324	179859.449537	35.913063
1321.472194	180159.383558	35.918080
1322.724227	180486.760754	35.923098
1323.703896	180798.827995	35.928116
1325.088237	181117.379336	35.933133
1326.487812	181431.906808	35.938151
1327.969977	181746.816024	35.943168
1329.192586	182053.253627	35.948186
1330.464291	182367.579443	35.953204
1331.568578	182678.837888	35.958221
1332.577292	183011.005458	35.963239
1334.467583	183319.371066	35.968256
1335.668859	183634.096872	35.973274
1336.525310	183937.001269	35.978292
1338.216267	184241.775092	35.983309
1339.181512	184558.385750	35.988327
1340.205909	184861.775383	35.993344
1341.415788	185173.678368	35.998362
1342.611640	185497.884867	36.003380
1344.126752	185808.573389	36.008397
1344.860552	186139.904560	36.013415
1346.110022	186468.322066	36.018432
1347.469285	186789.551769	36.023450
1348.482932	187123.482859	36.028468
1349.905442	187469.711786	36.033485
1350.900148	187821.433554	36.038503
1352.496435	188160.542465	36.043520
1353.760634	188505.394945	36.048538
1354.733658	188863.676686	36.053556
1356.516439	189206.632655	36.058573
1357.730835	189573.802714	36.063591
1359.067922	189928.489478	36.068608
1360.282372	190295.575277	36.073626
1361.474967	190663.098602	36.078644
1363.101896	191016.690584	36.083661
1364.175344	191408.750612	36.088679
1365.631993	191781.924379	36.093696
1366.652684	192159.691640	36.098714
1368.311108	192543.512853	36.103732
1369.854538	192907.120430	36.108749
1370.965408	193295.492593	36.113767
1372.534722	193675.666987	36.118784
1373.931330	194056.583163	36.123802
1375.156202	194434.673710	36.128820
1377.014258	194809.120198	36.133837
1378.633306	195196.049489	36.138855
1379.767357	195567.674794	36.143872
1381.540007	195961.057959	36.148890
1382.539697	196331.630864	36.153908
1384.342679	196709.195426	36.158925
1385.567014	197095.769875	36.163943
1386.764101	197476.066897	36.168960
1388.278693	197853.444570	36.173978
1389.169436	198250.491314	36.178996
1391.300499	198627.619385	36.184013
1392.817982	199017.064192	36.189031
1394.249346	199388.421255	36.194048
1396.148668	199773.173506	36.199066
1397.215465	200160.477593	36.204084
1399.356515	200528.892654	36.209101
1400.624764	200901.072145	36.214119
1402.288030	201264.453506	36.219136
1403.456500	201640.538511	36.224154
1404.478994	202016.624258	36.229172
1406.048194	202393.904148	36.234189
1407.585585	202769.388424	36.239207
1408.569232	203149.397169	36.244224
1410.189216	203513.863886	36.249242
1411.683145	203901.067572	36.254260
1413.152903	204277.370850	36.259277
1414.287023	204648.792426	36.264295
1415.431285	205036.440792	36.269312
1416.850573	205416.668910	36.274330
1417.644820	205804.442564	36.279348
1419.566613	206192.692408	36.284365
1421.333348	206585.490025	36.289383
1422.645141	206968.575239	36.294400
1424.066891	207364.379571	36.299418
1425.503017	207738.306117	36.304436
1427.152471	208133.899072	36.309453
1428.536982	208515.938812	36.314471
1429.847597	208880.863693	36.319488
1431.465675	209249.891623	36.324506
1432.948829	209603.414360	36.329524
1434.484908	209972.484564	36.334541
1435.695229	210337.483458	36.339559
1437.277863	210700.111557	36.344576
1438.406178	211067.958862	36.349594
1439.814596	211441.754991	36.354612
1440.908842	211816.417320	36.359629
1442.182276	212201.311747	36.364647
1443.492742	212580.208333	36.369664
1444.971025	212974.748400	36.374682
1445.755546	213364.833425	36.379700
1447.221702	213766.642485	36.384717
1448.915598	214161.634926	36.389735
1450.293419	214560.998744	36.394752
1452.080554	214952.525388	36.399770
1453.419339	215364.572269	36.404788
1454.986395	215771.300777	36.409805
1456.136826	216179.572890	36.414823
1457.281942	216590.362026	36.419840
1459.187943	217001.611560	36.424858
1460.563052	217413.941014	36.429876
1462.119973	217850.700168	36.434893
1463.172288	218316.751990	36.439911
1464.789915	218742.482568	36.444928
1466.377435	219161.768892	36.449946
1467.590657	219586.122188	36.454964
1469.629783	219997.895898	36.459981
1470.941866	220419.874390	36.464999
1472.427716	220859.274654	36.470016
1473.929156	221284.374872	36.475034
1475.614060	221715.897802	36.480052
1477.181078	222135.961748	36.485069
1478.418876	222559.840707	36.490087
1479.810172	223003.634151	36.495104
1481.690007	223425.150062	36.500122
1482.810050	223859.111536	36.505140
1484.552601	224281.034357	36.510157
1486.305934	224717.180590	36.515175
1487.740643	225144.948477	36.520192
1489.701550	225569.100595	36.525210
1490.961219	226000.354858	36.530228
1492.638561	226416.073378	36.535245
1494.034401	226847.943245	36.540263
1495.094382	227275.577502	36.545280
1497.150291	227707.443100	36.550298
1498.810779	228140.162854	36.555316
1500.459415	228572.860654	36.560333
1501.893714	228990.558376	36.565351
1503.076918	229414.902958	36.570368
1504.425065	229839.450301	36.575386
1505.651741	230280.224530	36.580404
1507.141304	230712.600051	36.585421
1508.936647	231163.011716	36.590439
1509.792356	231602.657602	36.595456
1511.258566	232028.919520	36.600474
1512.860974	232488.155931	36.605492
1514.054527	232940.984027	36.610509
1515.956150	233382.774243	36.615527
1517.603726	233837.282820	36.620544
1519.186774	234276.257897	36.625562
1520.296049	234743.888771	36.630580
1521.991574	235186.454818	36.635597
1523.597779	235636.022201	36.640615
1524.921674	236088.761782	36.645632
1526.628735	236538.441992	36.650650
1527.885294	236985.860788	36.655668
1529.680846	237423.285167	36.660685
1531.059666	237859.661724	36.665703
1532.177002	238287.242680	36.670720
1534.184010	238726.337266	36.675738
1535.571248	239173.739960	36.680756
1537.214894	239612.693356	36.685773
1538.820930	240042.864863	36.690791
1540.470992	240484.537164	36.695808
1541.698706	240921.529927	36.700826
1542.985734	241365.778840	36.705844
1544.964252	241819.135585	36.710861
1546.459032	242257.052318	36.715879
1547.914500	242708.287210	36.720896
1549.323311	243156.406205	36.725914
1550.626994	243617.320818	36.730932
1552.205399	244071.840371	36.735949
1553.909956	244531.928498	36.740967
1554.977634	244986.152949	36.745984
1557.320366	245445.451540	36.751002
1558.615356	245923.416917	36.756020
1560.077863	246389.619438	36.761037
1561.662277	246853.313137	36.766055
1562.954949	247332.475174	36.771072
1564.599001	247806.855061	36.776090
1566.239448	248294.267903	36.781108
1568.257826	248754.006185	36.786125
1570.211362	249221.452860	36.791143
1571.372773	249703.739150	36.796160
1573.562415	250146.735833	36.801178
1575.513192	250627.902330	36.806196
1577.145621	251085.751141	36.811213
1578.538420	251554.690308	36.816231
1579.640944	252021.366181	36.821248
1581.545199	252492.838429	36.826266
1583.120818	252973.713696	36.831284
1584.776371	253430.316203	36.836301
1586.208197	253906.872076	36.841319
1587.182244	254387.669980	36.846336
1588.958206	254866.506892	36.851354
1591.055731	255348.923732	36.856372
1592.570697	255825.289412	36.861389
1594.389760	256303.358008	36.866407
1595.938059	256794.350978	36.871424
1597.587496	257264.928659	36.876442
1599.147561	257753.125745	36.881460
1600.387346	258238.581483	36.886477
1602.377043	258713.091822	36.891495
1603.643509	259209.161986	36.896512
1605.301557	259686.496197	36.901530
1606.747507	260186.118755	36.906548
1608.352208	260683.403447	36.911565
1609.980841	261173.266422	36.916583
1611.592646	261662.598674	36.921600
1612.934009	262157.488005	36.926618
1614.672591	262650.203232	36.931636
1616.597514	263156.529162	36.936653
1618.313964	263651.813501	36.941671
1619.142722	264153.899781	36.946688
1621.085957	264649.095502	36.951706
1622.828010	265156.314509	36.956724
1624.231016	265663.589173	36.961741
1625.974043	266155.438476	36.966759
1627.599476	266659.271760	36.971776
1629.579002	267148.210793	36.976794
1631.410301	267662.196011	36.981812
1633.109883	268158.623540	36.986829
1634.628975	268642.861501	36.991847
1636.065898	269139.331443	36.996864
1637.784959	269619.572575	37.001882
1639.464148	270093.748455	37.006900
1640.954090	270572.171938	37.011917
1642.799902	271040.501976	37.016935
1644.078198	271531.127261	37.021952
1645.457628	271999.228243	37.026970
1647.116337	272501.322388	37.031988
1648.257817	272987.522757	37.037005
1650.011067	273487.034153	37.042023
1651.282391	273989.647206	37.047040
1653.179171	274499.141986	37.052058
1654.745460	275009.833534	37.057076
1656.228887	275513.552116	37.062093
1658.129521	276028.657502	37.067111
1659.675820	276537.317304	37.072128
1661.201343	277062.516537	37.077146
1663.026583	277579.612646	37.082164
1664.463002	278101.115601	37.087181
1666.434237	278622.249733	37.092199
1667.778255	279150.344758	37.097216
1669.691672	279676.718837	37.102234
1671.110105	280214.147008	37.107252
1672.227022	280756.627746	37.112269
1674.025038	281289.341910	37.117287
1675.749900	281849.119748	37.122304
1677.299829	282400.440608	37.127322
1678.976527	282945.540905	37.132340
1680.714376	283516.894833	37.137357
1682.445793	284073.591272	37.142375
1684.101405	284637.766487	37.147392
1685.569229	285194.731407	37.152410
1687.714802	285757.221746	37.157428
1689.113113	286318.868178	37.162445
1691.232251	286885.270728	37.167463
1692.777980	287456.185608	37.172480
1694.375655	288026.886572	37.177498
1696.676037	288574.634026	37.182516
1698.149779	289148.551615	37.187533
1700.788705	289712.647815	37.192551
1701.918465	290274.933286	37.197568
1703.527718	290834.114702	37.202586
1705.600919	291401.192982	37.207604
1707.162458	291967.972251	37.212621
1709.188125	292522.683616	37.217639
1710.578731	293101.093986	37.222656
1712.306043	293659.431013	37.227674
1713.779843	294227.764069	37.232692
1715.492639	294807.154703	37.237709
1717.530360	295371.249188	37.242727
1719.230624	295953.582638	37.247744
1721.383209	296527.126573	37.252762
1722.938983	297097.743576	37.257780
1724.674676	297668.226396	37.262797
1726.401272	298232.535829	37.267815
1728.193503	298808.565744	37.272832
1729.766775	299371.345189	37.277850
1732.114460	299941.105456	37.282868
1733.364347	300520.695089	37.287885
1735.065773	301081.844034	37.292903
1736.415037	301663.569612	37.297920
1738.499641	302231.303208	37.302938
1740.260983	302802.312372	37.307956
1741.842794	303387.418077	37.312973
1743.221001	303962.978942	37.317991
1745.009028	304555.256312	37.323008
1746.561689	305133.143156	37.328026
1748.206690	305719.061977	37.333044
1749.533789	306308.838980	37.338061
1751.732056	306880.614522	37.343079
1753.504383	307451.389978	37.348096
1754.657142	308030.898665	37.353114
1756.537750	308606.804108	37.358132
1758.089559	309170.239675	37.363149
1759.641052	309752.972345	37.368167
1761.233718	310345.801602	37.373184
1763.183247	310925.844591	37.378202
1765.019978	311523.627941	37.383220
1766.400130	312108.987784	37.388237
1768.174990	312728.053392	37.393255
1770.313072	313316.986887	37.398272
1771.772964	313921.493034	37.403290
1773.722230	314529.799008	37.408308
1775.429757	315127.982346	37.413325
1777.333523	315733.137247	37.418343
1779.268279	316357.428920	37.423360
1781.104609	316963.676770	37.428378
1783.033464	317565.866762	37.433396
1785.088894	318186.567725	37.438413
1786.836848	318798.858180	37.443431
1788.321054	319419.210858	37.448448
1790.288567	320035.339316	37.453466
1792.254869	320653.468429	37.458484
1794.046541	321284.316675	37.463501
1795.475404	321904.376630	37.468519
1797.253273	322515.562423	37.473536
1799.046160	323155.127407	37.478554
1801.314833	323772.365195	37.483572
1802.877769	324409.772146	37.488589
1804.809092	325037.844477	37.493607
1806.637030	325662.982381	37.498624
1808.118269	326315.186119	37.503642
1810.144229	326943.046047	37.508660
1811.814538	327598.785004	37.513677
1813.494415	328226.028751	37.518695
1815.151476	328881.908363	37.523712
1817.045064	329536.269231	37.528730
1818.846587	330181.015900	37.533748
1820.204129	330857.766824	37.538765
1822.319311	331508.083236	37.543783
1824.675698	332170.436923	37.548800
1826.125376	332844.991369	37.553818
1828.555390	333483.504485	37.558836
1830.076280	334151.760976	37.563853
1831.904675	334806.300917	37.568871
1833.618477	335470.016289	37.573888
1835.311906	336148.501360	37.578906
1837.553086	336803.609260	37.583924
1839.051387	337469.924922	37.588941
1841.008570	338139.862689	37.593959
1842.843152	338798.871513	37.598976
1844.771795	339489.713415	37.603994
1846.789378	340155.528524	37.609012
1848.866009	340823.863586	37.614029
1850.754633	341491.814754	37.619047
1852.595537	342160.424901	37.624064
1854.111544	342827.759829	37.629082
1855.869506	343498.548586	37.634100
1857.412079	344187.663882	37.639117
1859.456775	344856.203949	37.644135
1861.366431	345537.117566	37.649152
1863.084363	346220.185125	37.654170
1865.112172	346899.283233	37.659188
1867.216452	347588.079441	37.664205
1868.597091	348259.396949	37.669223
1871.151386	348940.637430	37.674240
1872.859602	349623.910826	37.679258
1874.590058	350265.575286	37.684276
1876.576277	350921.222530	37.689293
1878.233370	351584.832359	37.694311
1880.155738	352238.618378	37.699328
1881.803957	352900.941261	37.704346
1883.604819	353562.137853	37.709364
1885.329702	354221.154671	37.714381
1887.139442	354897.225368	37.719399
1889.452252	355571.172493	37.724416
1890.835446	356238.055910	37.729434
1892.634734	356919.272979	37.734452
1894.456525	357600.170889	37.739469
1896.197630	358297.716206	37.744487
1898.039267	358982.927263	37.749504
1899.943078	359682.046415	37.754522
1901.459782	360385.657710	37.759540
1903.444221	361090.219989	37.764557
1905.367532	361787.929811	37.769575
1907.521937	362504.161047	37.774592
1909.037247	363215.765945	37.779610
1911.248947	363937.137587	37.784628
1913.034484	364649.661575	37.789645
1914.958607	365381.886990	37.794663
1916.928416	366107.495219	37.799680
1918.340598	366847.362645	37.804698
1920.660380	367582.246229	37.809716
1922.559331	368313.405328	37.814733
1924.062015	369050.094882	37.819751
1926.143624	369795.831728	37.824768
1928.018416	370551.378966	37.829786
1929.950718	371290.388548	37.834804
1931.458742	372044.240910	37.839821
1933.537666	372807.723416	37.844839
1935.899154	373559.932525	37.849856
1937.628972	374324.505886	37.854874
1939.688252	375091.189770	37.859892
1941.901943	375861.078005	37.864909
1943.723512	376635.883547	37.869927
1946.404206	377381.796365	37.874944
1948.064806	378150.077170	37.879962
1950.582382	378907.041277	37.884980
1952.874658	379661.743564	37.889997
1954.628597	380413.804609	37.895015
1956.815937	381173.562477	37.900032
1958.559751	381923.613745	37.905050
1960.374732	382691.994973	37.910068
1962.269233	383448.453232	37.915085
1964.179757	384221.778555	37.920103
1966.094288	384986.819259	37.925120
1967.961773	385768.685307	37.930138
1970.044853	386533.763354	37.935156
1971.947460	387302.884251	37.940173
1973.527399	388082.586716	37.945191
1975.680314	388858.119291	37.950208
1977.525076	389648.565094	37.955226
1979.627199	390424.853531	37.960244
1981.576562	391216.636959	37.965261
1983.517653	391992.253911	37.970279
1985.752756	392769.830864	37.975296
1987.145848	393573.458412	37.980314
1989.212138	394350.592234	37.985332
1991.392861	395153.465259	37.990349
1992.637043	395950.160185	37.995367
1994.989787	396745.434568	38.000384
1997.070611	397560.273617	38.005402
1999.243967	398351.428814	38.010420
2001.159521	399152.692091	38.015437
2002.975536	399944.826456	38.020455
2005.176657	400709.582193	38.025472
2007.455853	401488.800290	38.030490
2009.270890	402260.674354	38.035508
2011.528308	403028.501622	38.040525
2013.132856	403811.822348	38.045543
2015.237401	404586.677182	38.050560
2016.911135	405355.069896	38.055578
2018.742478	406146.726036	38.060596
2020.984971	406936.949078	38.065613
2022.924244	407734.800438	38.070631
2025.151032	408530.275822	38.075648
2026.722641	409320.338635	38.080666
2028.364491	410121.057874	38.085684
2030.771863	410927.985856	38.090701
2032.471385	411742.631493	38.095719
2034.356625	412558.741702	38.100736
2036.635032	413369.392041	38.105754
2038.511834	414200.651799	38.110772
2040.705758	415030.364036	38.115789
2042.786820	415860.195349	38.120807
2044.829387	416686.283536	38.125824
2046.869235	417524.300146	38.130842
2049.069116	418351.601023	38.135860
2051.256104	419190.982814	38.140877
2053.195402	420032.859704	38.145895
2055.223200	420876.669387	38.150912
2057.297604	421726.267453	38.155930
2059.221609	422568.442414	38.160948
2061.663221	423425.569598	38.165965
2063.293620	424287.637195	38.170983
2065.673646	425147.221836	38.176000
2067.636819	426007.022483	38.181018
2069.724860	426859.886095	38.186036
2071.779630	427728.067121	38.191053
2073.471990	428606.858732	38.196071
2075.552324	429471.479480	38.201088
2078.082795	430356.650796	38.206106
2080.037885	431230.797239	38.211124
2082.535601	432107.960700	38.216141
2084.534516	432980.871032	38.221159
2086.831418	433850.105821	38.226176
2088.863467	434718.339637	38.231194
2090.945076	435599.946138	38.236212
2093.281048	436482.337573	38.241229
2095.202731	437358.032128	38.246247
2097.587332	438237.260828	38.251264
2099.618880	439114.135274	38.256282
2101.911112	439997.916516	38.261300
2103.957848	440872.341865	38.266317
2105.930761	441765.164597	38.271335
2108.367878	442630.854579	38.276352
2110.130099	443522.882694	38.281370
2112.443976	444406.587308	38.286388
2115.118208	445285.491783	38.291405
2116.970431	446168.695729	38.296423
2119.163501	447037.693065	38.301440
2121.427796	447919.189731	38.306458
2123.545905	448796.728834	38.311476
2126.125354	449670.716340	38.316493
2128.140272	450547.593841	38.321511
2130.055638	451427.031239	38.326528
2132.134050	452308.529543	38.331546
2133.783145	453189.353769	38.336564
2136.105864	454067.147293	38.341581
2138.054250	454959.327953	38.346599
2140.233652	455845.667388	38.351616
2142.216550	456735.945527	38.356634
2143.979797	457597.399496	38.361652
2146.758234	458478.318800	38.366669
2148.757507	459342.340267	38.371687
2150.894962	460191.235841	38.376704
2153.085610	461060.410689	38.381722
2155.114295	461923.204963	38.386740
2156.883704	462784.033386	38.391757
2159.185858	463659.547956	38.396775
2161.166053	464523.855553	38.401792
2163.491467	465401.361928	38.406810
2165.405807	466279.453025	38.411828
2167.718033	467159.764126	38.416845
2169.843607	468053.863367	38.421863
2171.913607	468933.174164	38.426880
2173.849141	469823.433086	38.431898
2175.875476	470727.532121	38.436916
2178.114413	471628.875517	38.441933
2180.082771	472547.349598	38.446951
2182.182934	473462.827248	38.451968
2184.190300	474385.702697	38.456986
2186.157798	475298.688346	38.462004
2188.036567	476255.998001	38.467021
2190.141462	477195.743497	38.472039
2192.568120	478136.146195	38.477056
2194.259112	479090.967071	38.482074
2196.270477	480057.605242	38.487092
2198.639342	481014.436906	38.492109
2200.778218	481988.073298	38.497127
2202.624654	482962.968320	38.502144
2204.934540	483955.256466	38.507162
2207.420857	484942.411681	38.512180
2209.668576	485934.247562	38.517197
2211.885714	486928.406376	38.522215
2214.173151	487925.628111	38.527232
2216.872031	488923.028777	38.532250
2219.102736	489914.392811	38.537268
2221.628238	490916.151242	38.542285
2223.582311	491920.672037	38.547303
2225.852146	492904.390111	38.552320
2228.334458	493898.766809	38.557338
2230.240730	494913.366849	38.562356
2232.745895	495905.050222	38.567373
2234.983242	496923.866787	38.572391
2237.279929	497927.829233	38.577408
2239.438169	498924.187214	38.582426
2241.679256	499945.545992	38.587444
2244.137121	500940.423608	38.592461
2246.030246	501960.556769	38.597479
2248.669517	502975.510877	38.602496
2250.636268	503983.553469	38.607514
2252.830063	505017.520972	38.612532
2255.116492	506026.243288	38.617549
2257.682947	507049.733425	38.622567
2259.775061	508080.044811	38.627584
2262.224703	509086.180952	38.632602
2264.416683	510124.211570	38.637620
2266.594100	511157.186592	38.642637
2268.772725	512176.584558	38.647655
2270.955328	513212.349859	38.652672
2273.286933	514248.325520	38.657690
2275.115394	515286.130782	38.662708
2277.713321	516321.674501	38.667725
2280.283674	517365.419201	38.672743
2282.434631	518402.864379	38.677760
2284.880602	519442.963102	38.682778
2286.781830	520478.597574	38.687796
2289.049441	521513.950997	38.692813
2291.659089	522562.629214	38.697831
2293.905751	523588.274213	38.702848
2296.260216	524603.758164	38.707866
2298.718783	525614.372066	38.712884
2300.974825	526613.065766	38.717901
2303.636413	527617.921534	38.722919
2306.056921	528606.635212	38.727936
2308.543851	529606.954780	38.732954
2310.729370	530608.062442	38.737972
2313.480848	531593.753830	38.742989
2316.018403	532583.643642	38.748007
2318.094565	533572.435437	38.753024
2320.469672	534573.242621	38.758042
2322.728584	535577.775442	38.763060
2325.307574	536569.452477	38.768077
2327.310465	537570.769143	38.773095
2329.404539	538581.462201	38.778112
2331.862732	539581.708589	38.783130
2333.931413	540616.919412	38.788148
2335.996573	541627.251487	38.793165
2338.101972	542659.238798	38.798183
2340.336238	543697.920956	38.803200
2342.731116	544724.025318	38.808218
2344.873978	545792.698917	38.813236
2346.743190	546836.490699	38.818253
2349.211473	547898.914302	38.823271
2351.200377	548976.321142	38.828288
2353.916352	550043.769417	38.833306
2356.342960	551126.015012	38.838324
2358.039938	552204.223372	38.843341
2360.490442	553290.718324	38.848359
2363.164736	554375.983895	38.853376
2365.226126	555482.072540	38.858394
2367.685625	556579.461121	38.863412
2369.814437	557682.141801	38.868429
2372.456282	558795.199862	38.873447
2374.575503	559926.641464	38.878464
2377.208834	561034.790900	38.883482
2379.469837	562161.748227	38.888500
2381.827029	563284.574880	38.893517
2384.054461	564403.107863	38.898535
2386.271391	565557.055979	38.903552
2388.618380	566691.997847	38.908570
2390.937789	567843.215560	38.913588
2393.284572	568984.936910	38.918605
2395.915218	570138.459658	38.923623
2397.786426	571295.568422	38.928640
2400.629978	572455.775540	38.933658
2403.127257	573621.154244	38.938676
2405.532646	574780.719650	38.943693
2408.286683	575944.186181	38.948711
2410.591486	577105.361262	38.953728
2413.479986	578267.587055	38.958746
2415.719370	579440.899376	38.963764
2418.235514	580593.588102	38.968781
2420.745699	581737.894197	38.973799
2423.250424	582918.257685	38.978816
2425.568369	584081.537572	38.983834
2428.145210	585250.481419	38.988852
2430.436269	586413.343547	38.993869
2433.375795	587578.544644	38.998887
2435.752805	588762.325420	39.003904
2438.258061	589909.827463	39.008922
2440.260525	591070.585371	39.013940
2442.721657	592234.062100	39.018957
2445.816246	593393.712963	39.023975
2447.882271	594572.761881	39.028992
2450.293837	595738.359405	39.034010
2452.861566	596900.409514	39.039028
2455.078055	598058.595725	39.044045
2457.661942	599208.643007	39.049063
2460.220287	600328.130859	39.054080
2462.594746	601466.420811	39.059098
2465.006466	602584.463487	39.064116
2467.340121	603709.871073	39.069133
2469.993509	604847.882168	39.074151
2472.116088	605996.880775	39.079168
2474.614344	607135.791455	39.084186
2476.672580	608286.972750	39.089204
2478.755543	609445.639854	39.094221
2481.516675	610596.470737	39.099239
2483.823906	611760.817916	39.104256
2486.500754	612913.777283	39.109274
2488.912864	614094.073931	39.114292
2491.240968	615275.810091	39.119309
2493.934824	616454.959761	39.124327
2496.240974	617653.750385	39.129344
2499.061453	618821.125320	39.134362
2501.251750	620023.327284	39.139380
2503.151053	621222.245965	39.144397
2505.917057	622432.386637	39.149415
2508.351955	623652.543059	39.154432
2510.768134	624867.917705	39.159450
2513.273066	626091.535563	39.164468
2515.415169	627327.164939	39.169485
2518.106384	628568.406316	39.174503
2520.328015	629812.877627	39.179520
2522.760059	631061.513963	39.184538
2525.569758	632322.076148	39.189556
2527.613069	633582.464498	39.194573
2530.210832	634852.595926	39.199591
2532.625920	636127.096537	39.204608
2535.079668	637405.029211	39.209626
2537.648590	638688.974707	39.214644
2539.892964	639996.069159	39.219661
2542.820048	641287.917096	39.224679
2545.249026	642591.409094	39.229696
2548.156525	643895.305101	39.234714
2550.335421	645188.132134	39.239732
2553.281495	646499.120646	39.244749
2555.966278	647809.534069	39.249767
2558.133126	649140.803092	39.254784
2560.999126	650447.603330	39.259802
2563.932031	651758.209903	39.264820
2566.290186	653084.438287	39.269837
2569.357820	654394.776060	39.274855
2571.932679	655720.069046	39.279872
2574.542729	657025.052247	39.284890
2577.436826	658347.797638	39.289908
2580.120993	659666.514670	39.294925
2582.738176	660963.900924	39.299943
2585.620894	662280.041153	39.304960
2588.672255	663599.758837	39.309978
2591.244513	664892.047622	39.314996
2593.717673	666199.160627	39.320013
2596.254429	667505.687252	39.325031
2598.813820	668817.256407	39.330048
2601.271531	670115.925929	39.335066
2604.437775	671420.021828	39.340084
2606.515616	672732.125252	39.345101
2609.459463	674034.256033	39.350119
2611.921724	675338.722416	39.355136
2614.634341	676645.601023	39.360154
2617.493928	677947.898226	39.365172
2619.947584	679244.265053	39.370189
2622.587102	680547.675668	39.375207
2625.214012	681867.202385	39.380224
2627.244012	683151.365013	39.385242
2630.000967	684442.083357	39.390260
2632.363500	685722.999624	39.395277
2634.981007	686985.915667	39.400295
2637.392008	688274.510108	39.405312
2639.822759	689549.811491	39.410330
2642.345318	690832.909635	39.415348
2644.837724	692134.690102	39.420365
2647.386111	693427.340030	39.425383
2649.837726	694745.024846	39.430400
2652.270955	696055.770923	39.435418
2655.168547	697371.703402	39.440436
2657.350287	698695.047198	39.445453
2659.906093	700013.568807	39.450471
2662.776891	701365.853060	39.455488
2665.113691	702712.811538	39.460506
2667.810564	704066.937745	39.465524
2669.773831	705426.227303	39.470541
2672.774019	706790.880760	39.475559
2675.173300	708170.726216	39.480576
2677.457619	709563.545597	39.485594
2680.338781	710960.052254	39.490612
2682.618194	712360.639128	39.495629
2684.975126	713764.102263	39.500647
2687.764893	715189.686206	39.505664
2690.390729	716615.948001	39.510682
2693.132069	718047.442402	39.515700
2695.666202	719495.351045	39.520717
2698.472217	720924.810210	39.525735
2701.125198	722398.958193	39.530752
2703.729280	723850.402825	39.535770
2706.985552	725304.798363	39.540788
2709.381596	726760.364787	39.545805
2712.273433	728241.786561	39.550823
2715.056410	729706.800100	39.555840
2717.632394	731187.049087	39.560858
2720.511784	732657.149048	39.565876
2723.041496	734141.807195	39.570893
2726.219167	735632.060742	39.575911
2729.054784	737122.884878	39.580928
2731.719966	738616.224404	39.585946
2734.443332	740115.987283	39.590964
2737.044518	741609.419079	39.595981
2739.821702	743103.823703	39.600999
2742.918442	744610.766780	39.606016
2745.566452	746091.852766	39.611034
2748.506532	747594.502595	39.616052
2751.181077	749115.146873	39.621069
2753.996604	750613.539720	39.626087
2757.159270	752105.624251	39.631104
2759.899136	753620.498392	39.636122
2762.822251	755116.475456	39.641140
2765.681853	756626.158229	39.646157
2768.541295	758125.154744	39.651175
2771.356049	759617.120378	39.656192
2774.085673	761123.868363	39.661210
2777.354254	762625.701208	39.666228
2780.190277	764128.979781	39.671245
2783.150656	765622.739747	39.676263
2786.000887	767110.565200	39.681280
2788.701673	768601.807189	39.686298
2791.459651	770084.286271	39.691316
2794.106749	771582.215747	39.696333
2797.207013	773081.733264	39.701351
2800.078665	774572.091513	39.706368
2802.721607	776064.297738	39.711386
2805.715464	777546.909980	39.716404
2808.014759	779049.859459	39.721421
2810.692009	780523.032182	39.726439
2813.821780	781986.506360	39.731456
2816.241767	783445.090868	39.736474
2819.154624	784892.947669	39.741492
2822.025867	786348.907263	39.746509
2824.712420	787803.963986	39.751527
2827.506588	789263.217337	39.756544
2830.116352	790728.917705	39.761562
2833.288566	792168.541727	39.766580
2836.158135	793649.523208	39.771597
2838.740824	795115.299265	39.776615
2841.754754	796578.886391	39.781632
2844.166911	798072.725388	39.786650
2847.402483	799535.706212	39.791668
2850.008681	801034.508805	39.796685
2852.772431	802529.780781	39.801703
2855.565214	804021.299831	39.806720
2857.989446	805529.824189	39.811738
2860.978055	807030.784234	39.816756
2863.467544	808559.073910	39.821773
2866.085975	810098.438844	39.826791
2869.266323	811628.663662	39.831808
2871.646487	813172.600374	39.836826
2874.497364	814720.161372	39.841844
2876.968352	816291.116054	39.846861
2879.481602	817853.542090	39.851879
2883.153894	819437.672148	39.856896
2885.913282	821025.675759	39.861914
2888.685385	822592.414794	39.866932
2891.535375	824200.185039	39.871949
2894.292937	825795.191719	39.876967
2897.494158	827395.296844	39.881984
2900.168311	829020.055542	39.887002
2903.025420	830625.471877	39.892020
2906.456602	832253.296421	39.897037
2909.016631	833863.759571	39.902055
2912.082454	835478.364506	39.907072
2914.713922	837121.554688	39.912090
2917.773928	838746.196901	39.917108
2920.313226	840388.175756	39.922125
2922.906093	842034.587832	39.927143
2926.049786	843675.181750	39.932160
2929.146030	845344.239504	39.937178
2931.768051	846999.810036	39.942196
2934.516965	848668.044805	39.947213
2937.517625	850341.527002	39.952231
2939.964514	852016.983612	39.957248
2943.146433	853718.768370	39.962266
2946.346426	855395.909255	39.967284
2949.052918	857082.188384	39.972301
2952.169524	858773.760503	39.977319
2955.055247	860459.569451	39.982336
2957.990492	862168.665653	39.987354
2960.950196	863872.043547	39.992372
2964.060365	865567.068424	39.997389
2967.022333	867284.511009	40.002407
2970.189735	868981.863503	40.007424
2972.923114	870698.273735	40.012442
2976.022983	872403.579404	40.017460
2978.939580	874117.429566	40.022477
2981.782480	875838.345607	40.027495
2985.503592	877537.143618	40.032512
2988.075407	879259.915091	40.037530
2991.544343	880970.337476	40.042548
2994.505285	882685.950705	40.047565
2997.065726	884387.600445	40.052583
3000.118428	886104.609785	40.057600
3002.992256	887827.031482	40.062618
3005.988756	889519.188864	40.067636
3008.964166	891209.599072	40.072653
3011.643469	892876.793059	40.077671
3014.939186	894559.989710	40.082688
3017.640613	896240.088713	40.087706
3020.686525	897920.792045	40.092724
3023.322290	899606.268862	40.097741
3026.273871	901297.742200	40.102759
3029.659881	902976.887437	40.107776
3031.907839	904691.051474	40.112794
3035.149915	906383.256907	40.117812
3038.175221	908092.688911	40.122829
3040.819169	909810.700088	40.127847
3043.927673	911540.410534	40.132864
3046.893479	913290.270240	40.137882
3049.550124	915022.904300	40.142900
3052.583733	916776.351911	40.147917
3055.693800	918532.201937	40.152935
3058.896839	920287.567124	40.157952
3061.750338	922060.177553	40.162970
3064.862400	923834.563586	40.167988
3067.937791	925609.331251	40.173005
3070.772002	927399.180822	40.178023
3074.107099	929183.270317	40.183040
3077.259724	930986.243759	40.188058
3079.903834	932796.352532	40.193076
3082.790273	934604.558907	40.198093
3085.794004	936431.748682	40.203111
3089.128077	938257.484661	40.208128
3091.901954	940093.103295	40.213146
3095.112897	941947.510756	40.218164
3098.188868	943785.892309	40.223181
3100.924448	945640.208448	40.228199
3104.230718	947494.148155	40.233216
3107.064690	949356.855750	40.238234
3109.676324	951222.265176	40.243252
3113.242507	953118.035642	40.248269
3116.175266	955008.213528	40.253287
3119.850083	956932.750896	40.258304
3122.416375	958880.397560	40.263322
3125.600597	960822.299255	40.268340
3128.643952	962771.388122	40.273357
3131.830735	964735.424733	40.278375
3135.223629	966681.959428	40.283392
3138.029598	968653.217154	40.288410
3141.145967	970616.622922	40.293428
3144.423331	972584.988901	40.298445
3147.367621	974562.291569	40.303463
3150.622976	976546.074941	40.308480
3154.035424	978532.945673	40.313498
3157.295917	980515.448844	40.318516
3160.659576	982496.467866	40.323533
3163.995379	984475.246122	40.328551
3167.370127	986460.630525	40.333568
3170.630848	988436.585709	40.338586
3173.748994	990414.115273	40.343604
3176.852085	992391.154062	40.348621
3179.696941	994376.294342	40.353639
3183.086993	996363.370880	40.358656
3185.952537	998348.380724	40.363674
3189.357494	1000349.013788	40.368692
3192.740082	1002356.998662	40.373709
3195.496817	1004341.186563	40.378727
3198.747996	1006333.615655	40.383744
3201.802696	1008333.032773	40.388762
3205.249034	1010341.464840	40.393780
3208.078614	1012335.041213	40.398797
3210.990163	1014352.109379	40.403815
3214.425427	1016336.420330	40.408832
3217.572992	1018307.593614	40.413850
3220.539328	1020277.911053	40.418868
3223.898391	1022230.257352	40.423885
3226.785250	1024199.112648	40.428903
3230.152786	1026157.822090	40.433920
3233.258730	1028127.964521	40.438938
3236.242655	1030106.220539	40.443956
3239.658220	1032087.759044	40.448973
3242.600542	1034086.331732	40.453991
3245.866446	1036056.447430	40.459008
3249.081789	1038068.788016	40.464026
3251.909958	1040075.547818	40.469044
3255.292955	1042071.373080	40.474061
3258.052077	1044096.349716	40.479079
3261.074115	1046127.476950	40.484096
3264.489924	1048162.030158	40.489114
3267.193785	1050211.829784	40.494132
3270.679551	1052275.938611	40.499149
3274.046491	1054346.891779	40.504167
3276.803318	1056430.912907	40.509184
3280.051219	1058516.659624	40.514202
3282.833040	1060610.337177	40.519220
3286.308534	1062731.233722	40.524237
3289.153384	1064849.304520	40.529255
3291.926813	1066976.643049	40.534272
3295.166998	1069107.107400	40.539290
3298.573826	1071261.638931	40.544308
3302.198709	1073430.809319	40.549325
3305.403184	1075586.545518	40.554343
3308.448841	1077752.946483	40.559360
3312.019351	1079929.407193	40.564378
3315.256623	1082118.734257	40.569396
3318.700310	1084297.010740	40.574413
3321.958626	1086501.401912	40.579431
3325.297698	1088702.592529	40.584448
3328.755309	1090904.303896	40.589466
3332.005866	1093105.632950	40.594484
3335.452347	1095322.927174	40.599501
3338.660718	1097542.214060	40.604519
3342.066456	1099739.102405	40.609536
3345.471956	1101971.412865	40.614554
3348.555145	1104204.472433	40.619572
3352.008540	1106429.117221	40.624589
3355.582014	1108664.056285	40.629607
3358.961924	1110896.385487	40.634624
3362.635385	1113136.394472	40.639642
3365.751231	1115376.891270	40.644660
3369.275856	1117596.901122	40.649677
3372.562530	1119839.779719	40.654695
3376.034656	1122074.470255	40.659712
3379.731448	1124313.979207	40.664730
3382.948870	1126550.445044	40.669748
3386.814003	1128789.659610	40.674765
3389.818178	1131031.581968	40.679783
3393.105253	1133269.670069	40.684800
3396.610439	1135521.556022	40.689818
3399.774731	1137772.826753	40.694836
3403.200569	1140018.082571	40.699853
3406.875612	1142275.400290	40.704871
3409.984132	1144519.366196	40.709888
3413.882735	1146768.770991	40.714906
3417.061031	1149020.548087	40.719924
3420.419979	1151268.878399	40.724941
3423.755876	1153522.294256	40.729959
3427.285444	1155777.355068	40.734976
3430.535597	1158025.646522	40.739994
3434.128307	1160277.726782	40.745012
3437.702175	1162508.532522	40.750016
3440.854134	1164686.980774	40.755021
3444.245236	1166815.961086	40.760026
3447.597833	1168868.024272	40.765031
3450.298290	1170850.435432	40.770036
3453.486605	1172752.618739	40.775040
3456.874787	1174597.142240	40.780045
3459.514459	1176340.972025	40.785050
3462.906944	1178013.068612	40.790055
3464.954331	1179602.734045	40.795060
3468.181915	1181109.439449	40.800064
3470.648175	1182555.034510	40.805069
3473.193127	1183919.108141	40.810074
3475.326889	1185198.606726	40.815079
3477.660337	1186420.671187	40.820084
3479.711654	1187564.453892	40.825088
3481.960572	1188673.921694	40.830093
3483.668219	1189687.093978	40.835098
3486.013458	1190644.521557	40.840103
3487.599630	1191528.708333	40.845108
3489.481816	1192363.941810	40.850112
3491.093302	1193130.990878	40.855117
3492.686214	1193847.029939	40.860122
3493.743031	1194514.794561	40.865127
3494.946432	1195154.188857	40.870132
3496.301175	1195716.125685	40.875136
3497.988442	1196254.949277	40.880141
3499.014558	1196744.175129	40.885146
3500.046181	1197181.549068	40.890151
3501.139673	1197606.019373	40.895156
3502.180480	1197971.910750	40.900160
3503.113359	1198305.329236	40.905165
3504.147869	1198612.720429	40.910170
3505.119686	1198883.889885	40.915175
3506.135059	1199113.290812	40.920180
3506.925587	1199329.303709	40.925184
3507.587365	1199498.894508	40.930189
3508.235661	1199655.536983	40.935194
3509.202146	1199779.385553	40.940199
3509.614137	1199881.748512	40.945204
3510.367978	1199953.099677	40.950208
3511.113196	1200017.885451	40.955213
3511.683964	1200044.617713	40.960218
3512.494880	1200052.738552	40.965223
3512.650678	1200060.592081	40.970228
3513.205402	1200029.172806	40.975232
3513.665406	1199976.664389	40.980237
3513.892767	1199910.123860	40.985242
3514.608641	1199833.183941	40.990247
3514.812047	1199742.725933	40.995252
3515.362755	1199629.696105	41.000256
3515.473029	1199512.139806	41.005261
3515.911218	1199375.858831	41.010266
3516.393934	1199228.403320	41.015271
3516.814335	1199073.261051	41.020276
3516.966851	1198905.774301	41.025280
3517.292043	1198730.278890	41.030285
3517.331659	1198546.661822	41.035290
3517.564709	1198347.149455	41.040295
3517.792079	1198150.351404	41.045300
3518.032644	1197934.870442	41.050304
3518.535837	1197714.176043	41.055309
3518.709892	1197481.983634	41.060314
3518.841612	1197238.338269	41.065319
3518.687487	1196997.450172	41.070324
3519.231287	1196751.555304	41.075328
3519.314380	1196489.955824	41.080333
3519.568508	1196225.780493	41.085338
3519.684296	1195953.259841	41.090343
3519.570445	1195679.166691	41.095348
3519.773939	1195400.406499	41.100352
3520.083501	1195122.928174	41.105357
3520.176273	1194828.663974	41.110362
3520.457265	1194523.459871	41.115367
3520.459066	1194236.782566	41.120372
3520.363940	1193921.557168	41.125376
3520.460041	1193622.903805	41.130381
3520.469413	1193312.977092	41.135386
3520.811503	1192996.683965	41.140391
3520.700321	1192691.060309	41.145396
3520.801443	1192360.584287	41.150400
3521.142391	1192037.187269	41.155405
3521.044855	1191711.869284	41.160410
3521.487856	1191376.200705	41.165415
3521.326908	1191049.442101	41.170420
3521.178624	1190713.639913	41.175424
3521.495036	1190374.074411	41.180429
3521.392920	1190027.882988	41.185434
3521.361079	1189674.043945	41.190439
3521.123246	1189337.133178	41.195444
3521.266297	1188978.800106	41.200448
3521.129677	1188651.509810	41.205453
3521.214128	1188301.787867	41.210458
3521.555914	1187954.538356	41.215463
3521.394044	1187599.074417	41.220468
3521.349084	1187251.371280	41.225472
3521.218509	1186903.470802	41.230477
3521.196553	1186544.149885	41.235482
3521.758464	1186189.316277	41.240487
3521.370257	1185844.960939	41.245492
3521.464001	1185478.869084	41.250496
3521.514973	1185118.026240	41.255501
3521.212763	1184756.275670	41.260506
3521.400479	1184393.102001	41.265511
3521.390728	1184035.580700	41.270516
3521.378604	1183673.800856	41.275520
3521.382845	1183313.404585	41.280525
3521.331272	1182955.439257	41.285530
3521.577515	1182585.071166	41.290535
3521.354417	1182224.542534	41.295540
3521.463729	1181844.355494	41.300544
3521.232813	1181494.037320	41.305549
3521.248123	1181124.073621	41.310554
3521.111671	1180752.037288	41.315559
3520.960894	1180392.216732	41.320564
3521.248341	1180032.393223	41.325568
3521.231351	1179668.828224	41.330573
3520.952991	1179310.554565	41.335578
3521.085203	1178939.850909	41.340583
3520.893608	1178577.085872	41.345588
3520.706265	1178206.570900	41.350592
3520.867795	1177851.986155	41.355597
3521.197731	1177490.943419	41.360602
3521.425388	1177112.086074	41.365607
3520.946176	1176747.262192	41.370612
3521.074285	1176375.905244	41.375616
3520.764872	1176013.640291	41.380621
3520.824185	1175651.949065	41.385626
3520.853467	1175283.074879	41.390631
3520.631505	1174918.551594	41.395636
3520.767445	1174553.001235	41.400640
3520.794514	1174192.062214	41.405645
3520.644854	1173824.999517	41.410650
3520.914489	1173447.659642	41.415655
3520.383636	1173090.413085	41.420660
3520.583663	1172718.406197	41.425664
3520.511250	1172361.599925	41.430669
3520.668305	1171993.508972	41.435674
3520.721787	1171626.257908	41.440679
3520.371747	1171258.481515	41.445684
3520.113371	1170901.039982	41.450688
3519.940017	1170549.597239	41.455693
3520.436118	1170186.133839	41.460698
3520.833729	1169819.736633	41.465703
3520.529452	1169455.599411	41.470708
3520.552476	1169082.796201	41.475712
3520.426961	1168712.538711	41.480717
3520.026360	1168355.606777	41.485722
3520.386803	1167985.312065	41.490727
3519.833097	1167623.447593	41.495732
3520.091019	1167266.143979	41.500736
3520.072287	1166911.127062	41.505741
3519.803361	1166551.029372	41.510746
3520.111078	1166183.070163	41.515751
3519.635371	1165821.162428	41.520756
3519.704961	1165455.362843	41.525760
3519.572836	1165107.890532	41.530765
3519.236613	1164756.179072	41.535770
3519.475006	1164385.271679	41.540775
3519.378643	1164044.806161	41.545780
3519.610790	1163689.907019	41.550784
3519.983304	1163336.661035	41.555789
3519.596516	1162977.470238	41.560794
3519.746966	1162610.230338	41.565799
3519.754160	1162257.822037	41.570804
3519.435484	1161899.490901	41.575808
3519.597612	1161541.717536	41.580813
3519.602047	1161193.490383	41.585818
3519.501953	1160828.907428	41.590823
3519.417237	1160482.254344	41.595828
3519.217299	1160117.449322	41.600832
3519.132212	1159766.779113	41.605837
3519.050135	1159428.563381	41.610842
3519.223775	1159064.474388	41.615847
3519.096852	1158719.602536	41.620852
3519.336358	1158373.513041	41.625856
3519.164053	1158003.166930	41.630861
3518.924940	1157664.674241	41.635866
3519.032489	1157311.065783	41.640871
3519.040324	1156966.529408	41.645876
3519.128960	1156612.782474	41.650880
3519.019888	1156263.773802	41.655885
3518.785857	1155908.424543	41.660890
3519.139651	1155541.980461	41.665895
3518.821988	1155208.640193	41.670900
3519.039281	1154846.143680	41.675904
3518.925385	1154508.373114	41.680909
3518.747545	1154170.307496	41.685914
3518.676056	1153819.332371	41.690919
3518.518851	1153462.764140	41.695924
3518.341317	1153119.331031	41.700928
3518.425167	1152760.403972	41.705933
3518.414236	1152429.581953	41.710938
3518.160735	1152088.365896	41.715943
3518.067142	1151746.344011	41.720948
3517.910854	1151413.588649	41.725952
3518.109303	1151081.605991	41.730957
3518.447547	1150755.734208	41.735962
3518.432218	1150400.166093	41.740967
3518.209845	1150066.105445	41.745972
3518.024619	1149723.209661	41.750976
3518.391073	1149369.971569	41.755981
3518.017225	1149046.195072	41.760986
3518.050671	1148696.566076	41.765991
3517.893889	1148357.365820	41.770996
3517.954308	1148028.055523	41.776000
3518.087348	1147676.731969	41.781005
3517.864222	1147353.963679	41.786010
3517.747635	1147018.650242	41.791015
3517.656644	1146686.438449	41.796020
3517.661162	1146353.810944	41.801024
3517.705026	1146018.502315	41.806029
3517.432526	1145690.712157	41.811034
3517.543231	1145350.326731	41.816039
3517.027842	1145036.848732	41.821044
3517.020591	1144706.678800	41.826048
3517.174294	1144375.418885	41.831053
3517.099628	1144064.939159	41.836058
3517.204898	1143729.190669	41.841063
3517.123209	1143420.191279	41.846068
3516.904660	1143085.593100	41.851072
3516.964211	1142760.221585	41.856077
3516.848477	1142450.127950	41.861082
3516.956570	1142123.191840	41.866087
3516.603377	1141807.408967	41.871092
3516.927602	1141489.029428	41.876096
3516.873744	1141172.874822	41.881101
3516.651480	1140852.744647	41.886106
3516.899305	1140529.386881	41.891111
3516.703999	1140206.366989	41.896116
3516.458221	1139887.510619	41.901120
3516.623508	1139584.508877	41.906125
3516.096447	1139268.128677	41.911130
3516.349078	1138951.885868	41.916135
3516.163300	1138642.244964	41.921140
3516.071791	1138338.644824	41.926144
3516.112571	1138033.866495	41.931149
3515.875151	1137724.275380	41.936154
3516.013606	1137419.065928	41.941159
3516.139593	1137124.568513	41.946164
3516.045523	1136817.653937	41.951168
3516.164983	1136499.672811	41.956173
3515.698095	1136194.872391	41.961178
3516.171553	1135891.513839	41.966183
3515.930032	1135583.887477	41.971188
3515.953007	1135283.512176	41.976192
3515.920769	1134980.089859	41.981197
3515.659925	1134682.766422	41.986202
3515.565763	1134378.940036	41.991207
3515.391789	1134078.908949	41.996212
3515.417364	1133777.213152	42.001216
3515.436904	1133475.501216	42.006221
3515.191090	1133189.111570	42.011226
3515.247505	1132888.785310	42.016231
3515.073058	1132600.927062	42.021236
3514.980400	1132319.691148	42.026240
3515.088302	1132025.768995	42.031245
3515.044245	1131734.041320	42.036250
3515.133940	1131451.018877	42.041255
3515.226858	1131164.749467	42.046260
3514.974017	1130876.905819	42.051264
3515.269311	1130579.451229	42.056269
3515.094048	1130294.795040	42.061274
3515.408017	1129987.038199	42.066279
3514.843805	1129707.357839	42.071284
3514.799813	1129428.622886	42.076288
3515.235268	1129132.775652	42.081293
3514.632279	1128852.961699	42.086298
3514.616426	1128565.619559	42.091303
3514.843069	1128273.372280	42.096308
3514.636590	1127998.392901	42.101312
3514.786477	1127704.985919	42.106317
3514.493612	1127431.988678	42.111322
3514.692888	1127140.634846	42.116327
3514.586166	1126859.778411	42.121332
3514.663070	1126568.984193	42.126336
3514.708317	1126290.165414	42.131341
3514.422263	1126014.050329	42.136346
3514.490096	1125725.875331	42.141351
3514.314391	1125454.660258	42.146356
3514.008205	1125179.932429	42.151360
3514.451733	1124889.842590	42.156365
3514.119298	1124613.662632	42.161370
3514.542669	1124336.772924	42.166375
3514.331905	1124067.967345	42.171380
3514.320538	1123791.501621	42.176384
3514.185841	1123509.521619	42.181389
3513.919571	1123241.064243	42.186394
3513.952845	1122959.122688	42.191399
3513.998402	1122693.251647	42.196404
3513.904945	1122420.440923	42.201408
3513.998599	1122155.963167	42.206413
3513.747908	1121888.768056	42.211418
3513.946229	1121618.819728	42.216423
3513.966216	1121348.506275	42.221428
3513.656818	1121078.328617	42.226432
3513.909167	1120804.711897	42.231437
3513.768634	1120544.668556	42.236442
3513.774141	1120273.065113	42.241447
3513.591779	1120001.478816	42.246452
3513.541005	1119737.286117	42.251456
3513.491751	1119465.555436	42.256461
3513.277614	1119213.650910	42.261466
3513.394046	1118946.724524	42.266471
3513.397062	1118691.330336	42.271476
3513.098845	1118430.066981	42.276480
3513.191522	1118162.819606	42.281485
3513.325114	1117898.029356	42.286490
3513.385490	1117642.099271	42.291495
3513.297666	1117393.804252	42.296500
3513.238859	1117125.100736	42.301504
3513.187059	1116864.101525	42.306509
3512.995297	1116615.596949	42.311514
3513.229372	1116356.908441	42.316519
3513.296087	1116091.372747	42.321524
3512.904466	1115836.193279	42.326528
3513.160986	1115587.662506	42.331533
3512.687278	1115335.808860	42.336538
3512.865700	1115070.490153	42.341543
3512.902566	1114831.207235	42.346548
3512.825686	1114573.532511	42.351552
3513.079535	1114307.782300	42.356557
3512.880155	1114079.659634	42.361562
3512.821302	1113818.227191	42.366567
3513.077062	1113563.977114	42.371572
3512.754203	1113324.686222	42.376576
3512.622055	1113069.618378	42.381581
3512.323376	1112815.614878	42.386586
3512.424406	1112567.446581	42.391591
3512.261274	1112333.807496	42.396596
3512.580382	1112088.919323	42.401600
3512.639793	1111840.342749	42.406605
3511.986726	1111597.881526	42.411610
3512.417383	1111359.332779	42.416615
3512.502856	1111110.527343	42.421620
3512.327996	1110861.944063	42.426624
3512.303569	1110615.423447	42.431629
3512.430978	1110385.849632	42.436634
3512.435888	1110138.061944	42.441639
3512.586138	1109890.238894	42.446644
3512.323048	1109658.217403	42.451648
3512.418652	1109407.804673	42.456653
3512.095105	1109164.988468	42.461658
3512.332022	1108922.927918	42.466663
3512.101958	1108678.165595	42.471668
3512.137017	1108444.897333	42.476672
3512.093508	1108200.464322	42.481677
3512.179120	1107966.498841	42.486682
3511.887130	1107715.784787	42.491687
3512.034461	1107485.797473	42.496692
3512.023606	1107242.270165	42.501696
3512.393948	1107010.698358	42.506701
3511.897241	1106780.309611	42.511706
3512.010099	1106533.197281	42.516711
3511.680645	1106304.574719	42.521716
3511.569050	1106069.413435	42.526720
3511.815457	1105834.564885	42.531725
3511.472526	1105607.060813	42.536730
3511.993476	1105362.883417	42.541735
3512.069468	1105147.419392	42.546740
3511.509614	1104912.281401	42.551744
3511.610670	1104666.040410	42.556749
3511.406763	1104446.105360	42.561754
3511.568000	1104212.059748	42.566759
3511.783376	1103984.968327	42.571764
3511.307383	1103757.885678	42.576768
3511.396602	1103528.598659	42.581773
3511.441925	1103314.785984	42.586778
3511.546752	1103082.133646	42.591783
3511.796977	1102857.855217	42.596788
3511.430414	1102623.636483	42.601792
3511.372094	1102398.052073	42.606797
3511.232452	1102164.827112	42.611802
3511.302726	1101941.017982	42.616807
3511.529040	1101725.487962	42.621812
3511.121232	1101500.114688	42.626816
3511.242182	1101273.784762	42.631821
3511.124052	1101054.748510	42.636826
3510.967926	1100833.415705	42.641831
3511.129531	1100619.094701	42.646836
3510.856832	1100402.638203	42.651840
3511.263015	1100188.068635	42.656845
3510.725665	1099962.365692	42.661850
3510.563629	1099735.922299	42.666855
3510.420379	1099528.778180	42.671860
3510.595378	1099328.839811	42.676864
3511.095669	1099104.172985	42.681869
3510.980679	1098901.971927	42.686874
3510.598698	1098669.209495	42.691879
3510.503052	1098451.115710	42.696884
3510.408361	1098241.714928	42.701888
3510.708212	1098041.038968	42.706893
3510.703624	1097824.339336	42.711898
3510.732384	1097620.249607	42.716903
3510.628314	1097410.339978	42.721908
3510.375374	1097198.629474	42.726912
3510.383778	1096985.145971	42.731917
3510.315877	1096785.536113	42.736922
3510.613205	1096564.144969	42.741927
3510.703532	1096358.371330	42.746932
3510.228195	1096155.839901	42.751936
3510.243185	1095936.956823	42.756941
3510.505675	1095734.001082	42.761946
3510.227548	1095530.361378	42.766951
3510.058696	1095332.245300	42.771956
3510.076345	1095118.495253	42.776960
3510.375837	1094913.780404	42.781965
3510.074897	1094714.610939	42.786970
3509.981112	1094506.787760	42.791975
3510.432406	1094312.838370	42.796980
3510.252065	1094107.597899	42.801985
3510.227271	1093897.634600	42.806989
3509.907466	1093697.282380	42.811994
3509.874063	1093488.261689	42.816999
3509.883990	1093290.137139	42.822004
3509.940864	1093090.561857	42.827009
3510.100000	1092900.917304	42.832013
3510.024413	1092711.974838	42.837018
3509.847327	1092510.310798	42.842023
3509.884849	1092310.614252	42.847028
3509.600493	1092116.420211	42.852033
3509.722143	1091914.876280	42.857037
3509.877288	1091731.605896	42.862042
3509.772921	1091514.957232	42.867047
3509.632478	1091323.200433	42.872052
3509.388184	1091140.933352	42.877057
3509.556740	1090943.558653	42.882061
3509.360390	1090769.123071	42.887066
3509.572245	1090576.803067	42.892071
3509.680777	1090372.235364	42.897076
3509.662646	1090178.023804	42.902081
3509.771094	1089996.809397	42.907085
3509.488385	1089811.247719	42.912090
3509.432327	1089599.590649	42.917095
3509.688353	1089409.041779	42.922100
3509.498293	1089236.854656	42.927105
3509.254042	1089035.551353	42.932109
3509.115475	1088851.753104	42.937114
3508.866745	1088674.576627	42.942119
3509.175251	1088484.657235	42.947124
3509.088821	1088308.879068	42.952129
3509.162134	1088130.194767	42.957133
3509.013988	1087942.918365	42.962138
3508.803050	1087755.262600	42.967143
3509.183387	1087572.964391	42.972148
3508.636177	1087405.760350	42.977153
3508.839785	1087230.186954	42.982157
3508.906838	1087052.809730	42.987162
3508.693550	1086866.752656	42.992167
3508.723518	1086692.244574	42.997172
3508.765442	1086513.033104	43.002177
3508.873798	1086338.500755	43.007181
3508.803039	1086173.001180	43.012186
3508.598902	1085990.746165	43.017191
3508.799705	1085809.280956	43.022196
3508.493207	1085648.979903	43.027201
3508.864594	1085465.845719	43.032205
3508.695994	1085291.900497	43.037210
3508.704025	1085108.430706	43.042215
3508.837285	1084946.215208	43.047220
3508.427625	1084772.772384	43.052225
3508.464472	1084587.842331	43.057229
3508.402206	1084431.395699	43.062234
3508.497413	1084269.262154	43.067239
3508.571264	1084081.911996	43.072244
3508.330518	1083920.782156	43.077249
3508.493564	1083749.417585	43.082253
3508.282093	1083590.382538	43.087258
3508.353171	1083422.282889	43.092263
3508.292243	1083240.583326	43.097268
3508.088195	1083079.134847	43.102273
3508.150626	1082925.117604	43.107277
3507.936514	1082764.524517	43.112282
3508.044013	1082603.394214	43.117287
3508.324928	1082431.393334	43.122292
3508.401723	1082276.875868	43.127297
3508.382098	1082100.310462	43.132301
3508.059395	1081952.467428	43.137306
3508.067749	1081783.560211	43.142311
3507.923403	1081622.921964	43.147316
3507.873330	1081469.265755	43.152321
3508.375698	1081296.041498	43.157325
3508.161588	1081139.045620	43.162330
3507.982872	1080977.818445	43.167335
3508.047685	1080812.996854	43.172340
3508.046030	1080651.730870	43.177345
3508.342488	1080491.178529	43.182349
3508.089514	1080326.010795	43.187354
3507.662913	1080157.316687	43.192359
3507.936330	1080004.525350	43.197364
3507.980889	1079845.530648	43.202369
3507.937416	1079684.818651	43.207373
3508.021869	1079529.166520	43.212378
3507.958907	1079361.347447	43.217383
3508.085640	1079215.563172	43.222388
3507.596464	1079049.436042	43.227393
3507.797897	1078881.078824	43.232397
3508.046335	1078739.964198	43.237402
3507.812733	1078576.851616	43.242407
3507.831643	1078413.212688	43.247412
3507.736222	1078281.164537	43.252417
3507.924435	1078120.080342	43.257421
3507.911336	1077965.359467	43.262426
3507.728240	1077804.231120	43.267431
3507.707447	1077638.271820	43.272436
3507.127607	1077487.182330	43.277441
3507.495652	1077349.659753	43.282445
3507.570170	1077205.462278	43.287450
3507.394750	1077045.462227	43.292455
3507.439027	1076897.037597	43.297460
3507.426524	1076760.714895	43.302465
3507.576729	1076601.608255	43.307469
3507.312953	1076444.965419	43.312474
3507.181431	1076294.345125	43.317479
3507.622492	1076150.539492	43.322484
3507.105402	1076011.016652	43.327489
3507.430679	1075861.749465	43.332493
3507.144307	1075712.194845	43.337498
3507.133573	1075572.865484	43.342503
3507.297276	1075433.215756	43.347508
3507.218187	1075280.350219	43.352513
3507.421884	1075136.364934	43.357517
3507.248992	1074994.454632	43.362522
3507.081441	1074845.432928	43.367527
3507.182953	1074699.916362	43.372532
3506.877892	1074558.400667	43.377537
3507.063963	1074417.568785	43.382541
3507.077092	1074278.394582	43.387546
3507.071585	1074134.417363	43.392551
3507.147852	1073981.682017	43.397556
3506.988279	1073851.650477	43.402561
3507.302960	1073712.220088	43.407565
3507.032447	1073568.079487	43.412570
3506.799142	1073427.099046	43.417575
3506.852517	1073294.329406	43.422580
3506.815597	1073153.789904	43.427585
3506.758609	1073010.944401	43.432589
3506.654459	1072873.483029	43.437594
3506.856643	1072752.396626	43.442599
3506.807744	1072599.258990	43.447604
3506.644018	1072471.597263	43.452609
3506.917758	1072344.148754	43.457613
3506.797732	1072208.498852	43.462618
3506.488396	1072079.026336	43.467623
3506.992137	1071931.832480	43.472628
3506.839867	1071792.045713	43.477633
3506.780017	1071660.408177	43.482637
3506.479034	1071530.056446	43.487642
3506.389555	1071394.573530	43.492647
3506.533125	1071261.547513	43.497652
3506.309659	1071144.916315	43.502657
3506.474099	1071011.015844	43.507661
3506.569171	1070877.219634	43.512666
3506.446337	1070759.890902	43.517671
3506.651957	1070622.802524	43.522676
3506.419546	1070484.725595	43.527681
3506.549915	1070360.906906	43.532685
3506.577928	1070232.873026	43.537690
3506.393394	1070098.142641	43.542695
3506.685365	1069964.003331	43.547700
3506.289998	1069860.542069	43.552705
3506.503111	1069719.296434	43.557709
3506.334502	1069589.549591	43.562714
3506.182559	1069459.412397	43.567719
3506.370321	1069328.447081	43.572724
3506.102568	1069204.667833	43.577729
3506.140826	1069080.739249	43.582733
3506.402718	1068959.463000	43.587738
3506.010802	1068845.214104	43.592743
3506.145343	1068710.493183	43.597748
3505.847225	1068596.415941	43.602753
3505.941099	1068482.752514	43.607757
3505.788272	1068351.339198	43.612762
3505.700847	1068232.700519	43.617767
3505.964823	1068117.751503	43.622772
3505.911862	1068011.987327	43.627777
3506.255100	1067880.961829	43.632781
3506.039245	1067774.065965	43.637786
3505.795539	1067663.903014	43.642791
3505.986085	1067538.856685	43.647796
3505.829138	1067424.154794	43.652801
3505.850937	1067300.958039	43.657805
3505.819800	1067163.437444	43.662810
3505.808954	1067062.552854	43.667815
3505.889004	1066943.666354	43.672820
3505.922879	1066834.883687	43.677825
3506.074891	1066707.708825	43.682829
3506.013210	1066594.224244	43.687834
3505.922891	1066483.242846	43.692839
3506.071567	1066343.459825	43.697844
3505.965325	1066237.958779	43.702849
3505.791569	1066120.923856	43.707853
3506.334093	1066000.978853	43.712858
3505.858895	1065874.561342	43.717863
3506.108334	1065755.140220	43.722868
3505.588296	1065643.346828	43.727873
3505.793312	1065519.598903	43.732877
3505.924986	1065417.025153	43.737882
3505.951146	1065301.286680	43.742887
3505.798689	1065184.035858	43.747892
3505.482692	1065072.197221	43.752897
3505.813679	1064946.972499	43.757901
3505.780598	1064837.584001	43.762906
3505.566449	1064732.360428	43.767911
3505.818661	1064610.701000	43.772916
3505.643442	1064503.734710	43.777921
3505.666935	1064391.056525	43.782925
3505.489458	1064281.295841	43.787930
3505.412582	1064177.097479	43.792935
3505.724532	1064052.913998	43.797940
3505.748905	1063952.640039	43.802945
3505.538646	1063825.169385	43.807949
3505.782965	1063728.223215	43.812954
3505.238080	1063612.543203	43.817959
3505.490343	1063498.654212	43.822964
3505.541989	1063404.813668	43.827969
3505.715233	1063292.569487	43.832973
3505.521948	1063182.885699	43.837978
3505.421299	1063079.055398	43.842983
3505.596391	1062959.104516	43.847988
3505.677293	1062859.860023	43.852993
3505.240524	1062754.057719	43.857997
3505.455990	1062647.183431	43.863002
3505.074715	1062529.913630	43.868007
3505.192341	1062425.072481	43.873012
3505.153711	1062336.522658	43.878017
3505.153478	1062208.113577	43.883021
3505.199816	1062116.754679	43.888026
3505.061092	1062015.990938	43.893031
3505.380932	1061891.949874	43.898036
3505.148145	1061810.065870	43.903041
3504.953422	1061696.020627	43.908045
3505.024457	1061600.605788	43.913050
3505.125346	1061516.544502	43.918055
3505.443968	1061406.452136	43.923060
3504.992091	1061306.208335	43.928065
3504.969712	1061202.522250	43.933069
3504.920700	1061102.882334	43.938074
3504.980108	1061007.747966	43.943079
3505.316032	1060901.205041	43.948084
3504.842114	1060800.666803	43.953089
3504.756968	1060692.648635	43.958093
3505.003450	1060603.542518	43.963098
3505.129986	1060504.825740	43.968103
3505.060552	1060399.495345	43.973108
3505.084382	1060305.606491	43.978113
3504.987847	1060201.432288	43.983117
3504.870258	1060115.748568	43.988122
3504.776175	1060014.074127	43.993127
3505.076719	1059901.932381	43.998132
3504.688279	1059814.169965	44.003137
3505.130854	1059714.809157	44.008141
3505.020759	1059616.789553	44.013146
3505.117796	1059530.387234	44.018151
3505.320589	1059423.741341	44.023156
3505.222245	1059325.907240	44.028161
3505.161727	1059222.767998	44.033165
3505.089605	1059116.931941	44.038170
3504.981338	1059028.244018	44.043175
3505.438232	1058917.982803	44.048180
3504.819982	1058830.724137	44.053185
3505.093925	1058729.446952	44.058189
3505.076489	1058615.982904	44.063194
3505.006180	1058523.427683	44.068199
3505.277406	1058425.613042	44.073204
3504.645174	1058331.413269	44.078209
3504.900054	1058236.776787	44.083213
3505.017915	1058141.390598	44.088218
3504.731382	1058032.679079	44.093223
3505.107919	1057939.173448	44.098228
3504.538153	1057857.286100	44.103233
3504.660308	1057752.451521	44.108237
3504.709669	1057658.802344	44.113242
3504.369324	1057573.404759	44.118247
3504.543734	1057490.136950	44.123252
3504.571715	1057392.247690	44.128257
3504.344103	1057302.202806	44.133261
3504.511510	1057214.500076	44.138266
3504.261214	1057140.835322	44.143271
3504.430095	1057041.085994	44.148276
3504.519881	1056954.548118	44.153281
3504.763891	1056872.126680	44.158285
3504.622750	1056778.301212	44.163290
3504.502730	1056684.856093	44.168295
3504.817119	1056598.179277	44.173300
3504.466516	1056520.475705	44.178305
3504.357168	1056414.786579	44.183309
3504.385379	1056338.463470	44.188314
3504.178708	1056238.279660	44.193319
3504.616458	1056159.959341	44.198324
3504.359182	1056079.535937	44.203329
3504.644548	1055990.059697	44.208333
3504.536706	1055894.189951	44.213338
3504.221449	1055821.481961	44.218343
3504.430813	1055727.773627	44.223348
3504.530576	1055645.743117	44.228353
3504.275945	1055556.734285	44.233357
3504.325360	1055470.854411	44.238362
3504.210902	1055400.710001	44.243367
3504.534548	1055303.602374	44.248372
3504.408918	1055221.602679	44.253377
3504.171035	1055138.945567	44.258381
3504.297466	1055053.142890	44.263386
3504.143078	1054967.288743	44.268391
3504.545359	1054895.607004	44.273396
3504.352809	1054810.335027	44.278401
3504.098955	1054727.674382	44.283405
3504.214073	1054652.470320	44.288410
3504.127100	1054576.334584	44.293415
3504.117074	1054492.859113	44.298420
3503.789653	1054419.941852	44.303425
3503.860712	1054330.377604	44.308429
3503.907230	1054254.119038	44.313434
3503.936864	1054192.322246	44.318439
3503.874817	1054094.774877	44.323444
3503.845515	1054022.188865	44.328449
3503.923180	1053952.380008	44.333453
3504.213307	1053869.424101	44.338458
3503.757931	1053794.784343	44.343463
3503.583493	1053717.397868	44.348468
3503.960235	1053659.876328	44.353473
3503.661258	1053568.721706	44.358477
3504.046608	1053505.026824	44.363482
3503.812243	1053435.359235	44.368487
3504.040158	1053352.791469	44.373492
3504.193958	1053277.851557	44.378497
3503.942547	1053203.266619	44.383501
3503.769891	1053126.450070	44.388506
3503.691740	1053046.435022	44.393511
3504.247121	1052972.389029	44.398516
3503.969425	1052905.903801	44.403521
3504.170980	1052823.043192	44.408525
3504.179695	1052753.037683	44.413530
3503.736302	1052673.655940	44.418535
3504.259977	1052581.578113	44.423540
3503.869549	1052523.013956	44.428545
3504.007435	1052437.843752	44.433549
3504.405883	1052352.340025	44.438554
3503.630666	1052286.411438	44.443559
3504.065407	1052195.306161	44.448564
3504.017658	1052129.738063	44.453569
3503.569923	1052053.337634	44.458573
3503.984072	1051990.488497	44.463578
3503.768485	1051909.708107	44.468583
3504.020795	1051835.311045	44.473588
3503.767940	1051774.691020	44.478593
3503.705035	1051691.857006	44.483597
3503.867114	1051618.436325	44.488602
3503.917455	1051549.469606	44.493607
3504.040736	1051470.073670	44.498612
3503.783871	1051402.120185	44.503617
3503.886136	1051329.380660	44.508621
3503.809860	1051255.029908	44.513626
3503.669832	1051173.261789	44.518631
3503.720991	1051103.710655	44.523636
3503.716687	1051036.096888	44.528641
3503.876760	1050958.520196	44.533645
3504.034367	1050889.913408	44.538650
3503.684769	1050824.765370	44.543655
3503.902776	1050742.160233	44.548660
3503.556690	1050674.308950	44.553665
3503.589937	1050595.590516	44.558669
3503.466707	1050534.163823	44.563674
3503.239139	1050457.801518	44.568679
3503.570865	1050387.037576	44.573684
3503.606196	1050330.019961	44.578689
3503.376042	1050265.424460	44.583693
3503.670808	1050198.330002	44.588698
3503.867002	1050129.803901	44.593703
3503.791653	1050054.375664	44.598708
3503.760104	1049980.289818	44.603713
3503.513850	1049902.475814	44.608717
3503.738072	1049841.852479	44.613722
3503.587998	1049775.308538	44.618727
3503.653219	1049709.307208	44.623732
3503.538298	1049643.141801	44.628737
3503.640093	1049571.440505	44.633741
3503.649636	1049501.490150	44.638746
3503.936310	1049451.561752	44.643751
3503.929506	1049363.859465	44.648756
3503.516343	1049294.940963	44.653761
3503.811368	1049215.677346	44.658765
3503.926769	1049149.854052	44.663770
3503.648743	1049081.586050	44.668775
3504.093886	1048998.917478	44.673780
3503.902378	1048933.335139	44.678785
3503.500642	1048854.953049	44.683789
3503.738621	1048796.052874	44.688794
3503.655936	1048731.415160	44.693799
3503.507360	1048657.041378	44.698804
3503.566071	1048593.054238	44.703809
3503.646590	1048515.649388	44.708813
3503.598347	1048451.485228	44.713818
3503.188603	1048392.108433	44.718823
3503.331039	1048318.357678	44.723828
3503.798200	1048264.142730	44.728833
3503.498908	1048191.138558	44.733837
3503.572827	1048119.809066	44.738842
3503.227187	1048056.847385	44.743847
3503.696911	1047992.206562	44.748852
3503.723056	1047926.865969	44.753857
3503.311454	1047859.183934	44.758861
3503.316970	1047784.869560	44.763866
3503.495107	1047729.635354	44.768871
3503.365243	1047663.545243	44.773876
3503.107210	1047605.872272	44.778881
3503.200680	1047545.148807	44.783885
3503.813990	1047491.577846	44.788890
3503.372407	1047418.297360	44.793895
3503.553956	1047349.063616	44.798900
3503.447369	1047279.104297	44.803905
3503.543867	1047222.623712	44.808909
3503.382964	1047152.864787	44.813914
3503.348267	1047084.532060	44.818919
3503.300771	1047026.432278	44.823924
3503.421121	1046975.350651	44.828929
3503.533373	1046906.122786	44.833933
3503.286909	1046833.864223	44.838938
3503.170174	1046777.317688	44.843943
3503.040772	1046701.369991	44.848948
3503.299516	1046658.757362	44.853953
3503.318097	1046595.719065	44.858957
3503.218906	1046526.328213	44.863962
3503.287582	1046465.886603	44.868967
3503.396040	1046412.871050	44.873972
3503.381115	1046347.615122	44.878977
3503.406788	1046277.428291	44.883981
3503.492655	1046219.394617	44.888986
3503.273367	1046156.004336	44.893991
3503.412022	1046094.195582	44.898996
3503.171896	1046036.213680	44.904001
3503.178916	1045971.722050	44.909005
3503.201637	1045921.708770	44.914010
3503.092263	1045864.475890	44.919015
3503.449048	1045795.966245	44.924020
3503.537929	1045742.850961	44.929025
3503.716601	1045681.899947	44.934029
3503.522627	1045603.051367	44.939034
3503.178624	1045549.715878	44.944039
3503.294004	1045483.269699	44.949044
3503.262647	1045415.108932	44.954049
3503.012437	1045354.418060	44.959053
3503.367806	1045300.482213	44.964058
3502.918559	1045245.036906	44.969063
3503.443204	1045188.754743	44.974068
3503.422511	1045128.313265	44.979073
3502.991527	1045062.531378	44.984077
3503.362071	1045004.244977	44.989082
3503.309364	1044943.903321	44.994087
3503.318276	1044877.853667	44.999092
3503.072953	1044819.570196	45.004097
3503.060851	1044762.792735	45.009101
3503.439202	1044691.368956	45.014106
3503.001377	1044635.625968	45.019111
3503.187405	1044581.517889	45.024116
3503.120972	1044521.367030	45.029121
3502.900852	1044461.530541	45.034125
3503.366274	1044404.381052	45.039130
3503.313528	1044346.060884	45.044135
3503.320034	1044288.889218	45.049140
3503.176331	1044232.321145	45.054145
3503.281204	1044171.655409	45.059149
3503.237334	1044109.371715	45.064154
3503.138525	1044057.719842	45.069159
3503.187689	1043996.095592	45.074164
3503.376904	1043938.793647	45.079169
3503.056105	1043865.349649	45.084173
3503.274956	1043809.586773	45.089178
3503.008720	1043763.368279	45.094183
3503.274808	1043695.233959	45.099188
3503.359105	1043632.054547	45.104193
3502.829039	1043582.304375	45.109197
3503.304958	1043519.059176	45.114202
3503.231032	1043462.085407	45.119207
3503.154894	1043387.532323	45.124212
3503.122681	1043337.021831	45.129217
3503.239707	1043288.031745	45.134221
3503.282252	1043239.053493	45.139226
3503.203017	1043173.770790	45.144231
3503.278696	1043105.660595	45.149236
3502.976323	1043059.248994	45.154241
3502.608902	1043004.443937	45.159245
3502.823488	1042945.002457	45.164250
3502.755849	1042894.203978	45.169255
3503.048278	1042831.947149	45.174260
3502.963038	1042776.417175	45.179265
3502.771272	1042736.746598	45.184269
3503.058223	1042681.154371	45.189274
3502.855584	1042619.363099	45.194279
3502.964531	1042563.316000	45.199284
3503.058064	1042515.578803	45.204289
3502.766705	1042469.160448	45.209293
3502.865379	1042409.056090	45.214298
3502.966730	1042367.788907	45.219303
3502.979558	1042302.674005	45.224308
3503.141549	1042252.604693	45.229313
3502.627066	1042201.487034	45.234317
3503.044380	1042136.110341	45.239322
3502.717345	1042100.901569	45.244327
3502.636129	1042047.778914	45.249332
3502.771345	1041995.103168	45.254337
3502.749658	1041957.427874	45.259341
3503.132212	1041902.198560	45.264346
3502.545504	1041853.891408	45.269351
3502.744103	1041792.507920	45.274356
3502.904399	1041753.835108	45.279361
3502.501730	1041696.510883	45.284365
3502.736993	1041648.259797	45.289370
3502.301261	1041602.437677	45.294375
3502.433718	1041551.980435	45.299380
3502.379900	1041511.312167	45.304385
3502.367365	1041471.216533	45.309389
3502.643901	1041409.815980	45.314394
3502.661322	1041370.777541	45.319399
3502.509271	1041327.515266	45.324404
3502.455680	1041279.308550	45.329409
3502.771852	1041230.460760	45.334413
3503.012348	1041178.532940	45.339418
3502.801523	1041132.090129	45.344423
3502.905314	1041088.107457	45.349428
3502.954490	1041042.490732	45.354433
3502.810630	1040987.145768	45.359437
3502.865229	1040933.313667	45.364442
3502.683193	1040883.481938	45.369447
3502.615360	1040829.379097	45.374452
3502.759557	1040790.895501	45.379457
3502.631704	1040742.696358	45.384461
3502.790587	1040681.307135	45.389466
3502.520005	1040651.491456	45.394471
3503.018550	1040590.915018	45.399476
3502.979541	1040538.930621	45.404481
3502.772484	1040482.528016	45.409485
3502.709811	1040423.878334	45.414490
3502.851282	1040380.367055	45.419495
3502.842478	1040330.695115	45.424500
3502.767117	1040285.382610	45.429505
3502.395361	1040235.189739	45.434509
3502.811131	1040184.576774	45.439514
3502.521544	1040141.037972	45.444519
3502.495376	1040097.068859	45.449524
3502.202710	1040043.478622	45.454529
3502.251429	1040016.216402	45.459533
3502.457907	1039977.233679	45.464538
3502.166404	1039929.730968	45.469543
3502.046088	1039889.738318	45.474548
3502.750250	1039848.933038	45.479553
3502.345190	1039814.205847	45.484557
3502.345924	1039753.025719	45.489562
3502.475837	1039719.176342	45.494567
3502.357903	1039664.780452	45.499572
3502.660723	1039620.463424	45.504577
3502.230046	1039595.114524	45.509581
3502.276498	1039546.103051	45.514586
3502.199168	1039510.643395	45.519591
3502.305538	1039464.714328	45.524596
3502.447347	1039424.288528	45.529601
3502.219535	1039392.139256	45.534605
3502.622731	1039355.342911	45.539610
3502.440930	1039310.716598	45.544615
3502.653606	1039256.455579	45.549620
3502.472411	1039224.974284	45.554625
3502.205990	1039178.717609	45.559629
3502.276058	1039135.788320	45.564634
3502.246046	1039108.437953	45.569639
3502.429318	1039056.209746	45.574644
3502.319515	1039017.949040	45.579649
3502.281601	1038983.929500	45.584653
3502.435405	1038933.831631	45.589658
3502.198211	1038897.911064	45.594663
3502.113424	1038852.491758	45.599668
3502.361515	1038807.693934	45.604673
3501.896460	1038776.546853	45.609677
3502.183377	1038726.231853	45.614682
3502.060913	1038704.211554	45.619687
3501.885769	1038659.965597	45.624692
3502.323766	1038629.635667	45.629697
3502.275453	1038591.748584	45.634701
3502.292924	1038541.186273	45.639706
3502.316460	1038523.298143	45.644711
3502.439029	1038468.850936	45.649716
3502.564366	1038414.789441	45.654721
3502.183568	1038376.665627	45.659725
3502.323763	1038334.105303	45.664730
3502.218413	1038298.255820	45.669735
3502.401715	1038257.427997	45.674740
3502.404608	1038219.143230	45.679745
3502.088872	1038175.980039	45.684749
3502.593492	1038141.189232	45.689754
3502.208940	1038109.735109	45.694759
3502.159562	1038064.303531	45.699764
3502.322710	1038024.250767	45.704769
3502.086904	1037988.517454	45.709773
3502.199524	1037951.759695	45.714778
3502.337994	1037924.569121	45.719783
3502.306485	1037882.807093	45.724788
3502.204789	1037840.766257	45.729793
3501.988994	1037802.514640	45.734797
3502.262292	1037763.021969	45.739802
3502.322819	1037719.503201	45.744807
3502.086331	1037675.646260	45.749812
3502.152237	1037630.192148	45.754817
3502.179311	1037591.899081	45.759821
3502.277583	1037480.399167	45.764826
3502.128763	1037323.008221	45.769831
3502.310549	1037096.419726	45.774836
3502.292408	1036818.215858	45.779841
3501.869153	1036497.416557	45.784845
3502.229582	1036081.592453	45.789850
3501.766616	1035611.320951	45.794855
3501.686017	1035099.061638	45.799860
3502.208118	1034493.879973	45.804865
3501.784973	1033838.669615	45.809869
3501.977504	1033103.254773	45.814874
3501.310317	1032320.365274	45.819879
3501.174581	1031442.612448	45.824884
3501.490060	1030504.236552	45.829889
3500.841749	1029520.739269	45.834893
3500.935969	1028428.670915	45.839898
3500.349071	1027297.851048	45.844903
3500.540108	1026087.225806	45.849908
3500.623517	1024779.348500	45.854913
3499.841955	1023416.636760	45.859917
3500.095399	1021957.432767	45.864922
3499.559025	1020417.189144	45.869927
3499.346912	1018821.267843	45.874932
3499.287701	1017126.465643	45.879937
3498.775884	1015366.575278	45.884941
3498.350680	1013514.063368	45.889946
3497.792877	1011591.703038	45.894951
3497.801093	1009590.076884	45.899956
3497.169621	1007488.983065	45.904961
3496.890232	1005321.114982	45.909965
3496.783840	1003068.720290	45.914970
3496.319843	1000745.022984	45.919975
3495.941869	998347.916077	45.924980
3495.547640	995839.432091	45.929985
3495.128084	993274.196178	45.934989
3494.545774	990618.128389	45.939994
3494.112208	987892.707516	45.944999
3493.678273	985057.358703	45.950004
3493.066300	982162.529897	45.955009
3492.641189	979181.792883	45.960013
3492.128181	976112.910875	45.965018
3491.114943	972985.544841	45.970023
3490.904984	969772.476980	45.975028
3490.495893	966469.130280	45.980033
3489.871851	963100.141946	45.985037
3489.232320	959624.881922	45.990042
3488.419730	956098.020486	45.995047
3487.640087	952538.969580	46.000052
3487.272697	948919.992384	46.005057
3486.199931	945257.582515	46.010061
3485.625530	941493.375168	46.015066
3484.151341	937661.266159	46.020071
3483.651655	933760.147803	46.025076
3482.741718	929774.554415	46.030081
3482.441750	925711.556373	46.035085
3481.681230	921573.297380	46.040090
3480.951289	917347.609885	46.045095
3480.001681	913041.974400	46.050100
3479.447349	908664.812826	46.055105
3477.988875	904201.722638	46.060109
3477.671769	899658.183984	46.065114
3476.498426	895050.320241	46.070119
3475.339681	890350.193715	46.075124
3474.495575	885581.390660	46.080129
3473.695698	880732.292557	46.085133
3472.279890	875800.716472	46.090138
3471.357892	870793.404109	46.095143
3470.636764	865716.866497	46.100148
3469.626080	860546.452638	46.105153
3467.884129	855308.617966	46.110157
3467.299777	849991.922313	46.115162
3465.827016	844597.236989	46.120167
3464.966175	839128.511850	46.125172
3463.623520	833560.253484	46.130177
3462.393232	827953.945805	46.135181
3461.409000	822240.016376	46.140186
3460.144166	816452.119663	46.145191
3458.636065	810575.225992	46.150196
3457.633250	804643.626436	46.155201
3456.273930	798622.096358	46.160205
3455.122938	792527.233492	46.165210
3453.747507	786357.370896	46.170215
3452.404231	780090.004318	46.175220
3451.310454	773760.096191	46.180225
3449.903045	767366.230108	46.185229
3448.475929	760863.620232	46.190234
3446.812576	754298.434188	46.195239
3445.538447	747660.562883	46.200244
3444.173753	740943.906999	46.205249
3442.780821	734145.181640	46.210253
3441.107953	727258.371184	46.215258
3439.496591	720311.319576	46.220263
3437.946547	713266.750426	46.225268
3436.522480	706160.930678	46.230273
3434.904918	698971.346926	46.235277
3433.372437	691711.940991	46.240282
3431.889241	684388.937698	46.245287
3429.845097	676964.222662	46.250292
3428.687565	669492.601088	46.255297
3426.636956	661940.232909	46.260301
3424.811982	654299.425455	46.265306
3423.064625	646601.774242	46.270311
3421.324774	638828.778883	46.275316
3419.625204	630967.678985	46.280321
3417.595782	623056.909405	46.285325
3415.818340	615071.632703	46.290330
3414.102284	607025.058821	46.295335
3412.031092	598885.583997	46.300340
3410.290990	590696.666594	46.305345
3408.524758	582433.473162	46.310349
3406.280869	574084.558557	46.315354
3404.148270	565683.347144	46.320359
3402.172649	557209.887406	46.325364
3400.403425	548665.003403	46.330369
3398.140591	540065.238963	46.335373
3395.808162	531380.155931	46.340378
3393.764376	522647.545422	46.345383
3391.255292	513853.525783	46.350388
3389.314972	504987.939378	46.355393
3386.752623	496075.936849	46.360397
3384.518867	487085.229791	46.365402
3382.469383	478041.279568	46.370407
3380.133971	468931.862155	46.375412
3377.591686	459764.819613	46.380417
3375.370196	450549.107244	46.385421
3372.971601	441262.010873	46.390426
3370.177994	431925.147165	46.395431
3367.792516	422539.062158	46.400436
3365.541922	413078.328294	46.405441
3362.576738	403572.659849	46.410445
3359.721191	393999.040125	46.415450
3357.181984	384397.141867	46.420455
3354.290737	374749.724890	46.425460
3351.403839	365045.494920	46.430465
3348.445849	355316.268516	46.435469
3345.770383	345522.883573	46.440474
3342.693037	335685.952569	46.445479
3339.563358	325818.481703	46.450484
3336.738263	315906.885028	46.455489
3333.408724	305972.954257	46.460493
3330.536683	295966.623637	46.465498
3327.109120	285961.983185	46.470503
3323.423043	275923.116362	46.475508
3320.363147	265822.537528	46.480513
3316.891770	255734.369755	46.485517
3313.712617	245590.749512	46.490522
3310.229535	235431.914408	46.495527
3306.375627	225224.546420	46.500532
3302.959235	214955.365003	46.505537
3298.716455	204746.821832	46.510541
3295.309309	194514.803620	46.515546
3290.984919	184271.388885	46.520551
3286.762850	174030.585568	46.525556
3282.816949	163781.599800	46.530561
3278.406038	153531.004909	46.535565
3274.116997	143274.890799	46.540570
3269.236518	133026.139679	46.545575
3264.150132	122803.306857	46.550580
3259.563825	112600.102671	46.555585
3254.127364	102428.140237	46.560589
3248.643430	92273.067708	46.565594
3243.103327	82161.747876	46.570599
3237.042467	72077.402295	46.575604
3230.796325	62060.802286	46.580609
3224.118927	52124.452477	46.585613
3216.343024	42259.734790	46.590618
3207.671110	32506.357857	46.595623
3193.124957	23012.622870	46.600628
3162.122987	14141.563068	46.605633
3119.984140	5954.668765	46.610637
2993.681399	665.135297	46.615642
2736.638600	412.411991	46.620647
2585.656248	413.441963	46.625652
2560.778406	359.849755	46.630657
2621.902972	351.990851	46.635661
2716.285376	341.042279	46.640666
2800.792041	360.241343	46.645671
2854.802503	372.304842	46.650676
2877.874449	342.755681	46.655681
2877.063403	348.585512	46.660685
2865.027419	331.437859	46.665690
2850.274535	328.126903	46.670695
2838.269913	335.510142	46.675700
2831.187140	328.995413	46.680705
2827.624265	340.804184	46.685709
2826.226974	325.834863	46.690714
2825.896891	315.940322	46.695719
2824.946726	319.798500	46.700724
2823.317866	317.900556	46.705729
2820.632682	327.316689	46.710733
2817.361766	326.791373	46.715738
2814.243293	315.109976	46.720743
2810.709656	316.060892	46.725748
2808.064839	307.291756	46.730753
2804.758128	311.955764	46.735757
2801.772067	311.886258	46.740762
2798.605386	311.434532	46.745767
2795.274346	313.258528	46.750772
2792.383878	307.740934	46.755777
2789.070175	310.577861	46.760781
2785.693433	308.012782	46.765786
2782.848224	306.071991	46.770791
2779.445692	305.240452	46.775796
2776.525801	296.437858	46.780801
2773.155031	307.078603	46.785805
2769.436140	300.194442	46.790810
2766.385167	304.160912	46.795815
2762.701727	314.388337	46.800820
2759.707653	300.659731	46.805825
2756.598346	290.471842	46.810829
2753.364345	302.065772	46.815834
2749.917557	294.235322	46.820839
2746.300523	298.974288	46.825844
2742.856651	294.384385	46.830849
2739.814346	291.051780	46.835853
2736.195663	295.980346	46.840858
2732.748444	288.456806	46.845863
2729.153661	293.737097	46.850868
2725.783914	286.065233	46.855873
2722.823845	293.112524	46.860877
2719.874461	298.648389	46.865882
2716.385463	282.801144	46.870887
2712.440566	291.642913	46.875892
2709.353817	279.928842	46.880897
2705.803916	288.313419	46.885901
2701.900245	283.552507	46.890906
2699.214765	278.449865	46.895911
2695.374241	284.038540	46.900916
2692.317856	275.749820	46.905921
2688.994306	273.722094	46.910925
2685.145842	277.206618	46.915930
2681.742084	275.173374	46.920935
2678.435715	282.284283	46.925940
2675.437857	276.124929	46.930945
2671.533629	278.824752	46.935949
2667.652796	280.278516	46.940954
2664.216540	279.759417	46.945959
2661.346053	277.628588	46.950964
2658.296304	277.148862	46.955969
2654.634013	272.589498	46.960973
2650.989007	277.481294	46.965978
2647.405321	274.273710	46.970983
2643.964170	279.612954	46.975988
2640.777927	274.450145	46.980993
2636.797351	273.830398	46.985997
2633.019510	278.498938	46.991002
2630.380024	267.154345	46.996007
2626.602818	279.650902	47.001012
2622.800283	270.120314	47.006017
2619.829520	271.603798	47.011021
2616.138642	266.696665	47.016026
2612.259450	260.714039	47.021031
2608.727758	269.865665	47.026036
2605.826026	267.994549	47.031041
2602.304549	260.875502	47.036045
2599.237569	269.112802	47.041050
2596.230510	266.447102	47.046055
2592.056002	268.429001	47.051060
2588.897767	270.322058	47.056065
2585.627034	267.881370	47.061069
2581.658017	255.381927	47.066074
2578.243114	265.241413	47.071079
2574.663413	257.739423	47.076084
2571.016072	268.803672	47.081089
2567.684636	264.888497	47.086093
2564.310368	261.731370	47.091098
2561.176374	263.435358	47.096103
2557.256921	257.543953	47.101108
2554.226094	256.618768	47.106113
2550.194495	259.896277	47.111117
2546.896818	250.955838	47.116122
2543.472064	263.709408	47.121127
2539.825499	265.662190	47.126132
2536.390995	259.244108	47.131137
2533.143463	263.718988	47.136141
2529.417001	257.619473	47.141146
2526.323886	258.094363	47.146151
2522.716798	253.270350	47.151156
2519.058678	243.091326	47.156161
2515.232078	245.712022	47.161165
2511.878061	252.763451	47.166170
2509.000235	244.551254	47.171175
2505.488949	243.920983	47.176180
2501.988459	243.243551	47.181185
2497.778685	254.037008	47.186189
2494.549271	256.541283	47.191194
2491.174120	247.930835	47.196199
2487.598152	245.607026	47.201204
2484.316551	248.407102	47.206209
2480.796405	256.785064	47.211213
2477.314418	254.134692	47.216218
2473.818887	241.461750	47.221223
2470.464703	247.682325	47.226228
2466.798197	241.280149	47.231233
2463.477712	236.752831	47.236237
2459.808734	246.701896	47.241242
2456.311798	237.863333	47.246247
2452.403104	242.857585	47.251252
2449.448621	243.800861	47.256257
2445.695940	245.553446	47.261261
2442.430472	247.537940	47.266266
2439.097179	244.179172	47.271271
2435.342007	243.128225	47.276276
2432.117679	239.697922	47.281281
2428.591570	244.312304	47.286285
2424.915944	239.503398	47.291290
2421.654864	237.489077	47.296295
2417.859829	253.033498	47.301300
2414.548221	234.978483	47.306305
2411.289546	241.096804	47.311309
2407.675859	237.431593	47.316314
2403.937415	233.857500	47.321319
2400.191583	236.159880	47.326324
2397.314311	231.544014	47.331329
2393.374701	244.388443	47.336333
2389.696050	232.883773	47.341338
2386.509578	240.522051	47.346343
2383.009983	238.413500	47.351348
2379.820920	225.842611	47.356353
2376.370616	227.987544	47.361357
2372.792997	232.662236	47.366362
2369.071445	223.334831	47.371367
2365.956849	241.764649	47.376372
2361.966095	237.656224	47.381377
2358.416021	227.659565	47.386381
2354.787061	236.678334	47.391386
2351.482136	223.786103	47.396391
2347.999110	231.984245	47.401396
2344.478937	226.414061	47.406401
2341.019280	229.208238	47.411405
2337.777933	230.511116	47.416410
2334.435989	222.402489	47.421415
2330.633734	235.170513	47.426420
2327.598089	221.276812	47.431425
2324.029292	228.481321	47.436429
2319.977379	228.561646	47.441434
2316.871287	223.746777	47.446439
2312.761644	237.828616	47.451444
2309.498963	237.123696	47.456449
2305.925966	233.069826	47.461453
2302.602922	237.673755	47.466458
2299.423745	227.573833	47.471463
2295.840507	232.928642	47.476468
2292.526854	219.604289	47.481473
2288.919546	227.048882	47.486477
2284.759580	227.523326	47.491482
2281.797734	230.230985	47.496487
2278.094111	229.417372	47.501492
2274.757418	225.485458	47.506497
2271.229475	231.413235	47.511501
2267.703407	226.099784	47.516506
2264.473757	219.444939	47.521511
2260.715200	231.941279	47.526516
2257.067821	230.258009	47.531521
2253.816201	223.001430	47.536525
2250.639520	225.025716	47.541530
2247.071993	219.316496	47.546535
2243.245718	230.828263	47.551540
2239.653757	226.892493	47.556545
2236.330515	220.047497	47.561549
2232.555039	228.185885	47.566554
2229.082212	219.886099	47.571559
2225.655246	215.459142	47.576564
2222.447877	216.618047	47.581569
2218.726532	215.610173	47.586573
2214.946441	218.163552	47.591578
2211.765914	217.134849	47.596583
2208.322865	225.576739	47.601588
2204.877751	210.044574	47.606593
2201.853580	217.706252	47.611597
2197.852888	226.482131	47.616602
2194.404266	219.308984	47.621607
2190.708054	225.095054	47.626612
2187.216323	214.481447	47.631617
2183.970195	209.562081	47.636621
2179.913727	212.293559	47.641626
2176.358789	207.678090	47.646631
2172.846349	225.044225	47.651636
2169.559379	211.732815	47.656641
2166.421259	221.261940	47.661645
2163.506077	210.311442	47.666650
2159.898971	208.575312	47.671655
2155.766388	219.797164	47.676660
2152.243549	205.193199	47.681665
2148.892005	216.634579	47.686669
2145.105694	217.473665	47.691674
2141.794567	207.437732	47.696679
2138.375223	216.619904	47.701684
2134.906732	207.068786	47.706689
2131.773933	206.825154	47.711693
2127.900562	211.613646	47.716698
2124.204891	205.379568	47.721703
2120.939475	220.417306	47.726708
2117.217345	211.276715	47.731713
2114.081004	211.591383	47.736717
2109.819222	216.548629	47.741722
2106.751225	202.327043	47.746727
2103.482475	209.570732	47.751732
2099.804877	209.610249	47.756737
2096.486571	208.394777	47.761741
2092.802615	208.892917	47.766746
2089.260889	212.453985	47.771751
2085.614068	211.504722	47.776756
2082.159296	201.663494	47.781761
2079.066208	209.203093	47.786765
2075.180363	209.067525	47.791770
2071.898607	205.591526	47.796775
2068.216985	205.795788	47.801780
2064.673577	198.618529	47.806785
2061.228833	198.922333	47.811789
2057.651797	209.413774	47.816794
2054.540591	207.656174	47.821799
2050.732139	208.788222	47.826804
2047.317097	216.117827	47.831809
2044.223789	196.842410	47.836813
2040.327282	213.760785	47.841818
2037.094936	194.860615	47.846823
2033.056143	208.231178	47.851828
2029.563024	197.925418	47.856833
2026.135679	197.999754	47.861837
2022.729817	214.624395	47.866842
2019.412138	197.555572	47.871847
2016.258612	196.763325	47.876852
2012.490715	206.084428	47.881857
2009.295813	199.147552	47.886861
2005.227491	205.937946	47.891866
2001.996739	199.538355	47.896871
1998.014812	197.554852	47.901876
1994.676595	206.252502	47.906881
1991.356711	193.690714	47.911885
1987.875945	202.402114	47.916890
1984.401395	203.775576	47.921895
1980.606218	200.066745	47.926900
1977.484908	197.056326	47.931905
1974.355845	199.405538	47.936909
1970.391507	208.453230	47.941914
1966.775043	191.593070	47.946919
1963.172520	198.988060	47.951924
1959.891239	203.081485	47.956929
1956.102607	197.894695	47.961933
1952.628780	206.226221	47.966938
1949.617674	190.819163	47.971943
1946.031256	194.806166	47.976948
1942.491627	199.338325	47.981953
1938.893014	194.650478	47.986957
1935.002005	195.177725	47.991962
1931.699474	196.782399	47.996967
1928.044663	199.202974	48.001972
1924.626817	207.200696	48.006977
1921.770732	191.014045	48.011981
1917.849195	204.193644	48.016986
1914.212461	189.701768	48.021991
1910.349093	204.168616	48.026996
1906.864931	203.636171	48.032001
1903.677499	199.819520	48.037005
1900.182335	203.540113	48.042010
1897.087964	194.009600	48.047015
1893.366276	194.168667	48.052020
1889.803526	192.529541	48.057025
1886.616962	192.629528	48.062029
1882.954486	200.073018	48.067034
1879.346746	196.162842	48.072039
1875.858567	199.209157	48.077044
1872.241812	198.926008	48.082049
1869.122108	184.817287	48.087053
1865.152539	193.927443	48.092058
1861.669469	186.971502	48.097063
1858.192927	192.240316	48.102068
1854.316215	199.185233	48.107073
1851.262256	191.151607	48.112077
1847.459064	197.359961	48.117082
1844.709077	192.063633	48.122087
1840.815293	187.395043	48.127092
1837.152648	191.582316	48.132097
1834.431198	186.641679	48.137101
1830.224283	197.323840	48.142106
1826.610066	187.018359	48.147111
1823.058690	195.379694	48.152116
1819.547166	193.928873	48.157121
1816.576115	189.481173	48.162125
1812.778482	197.475495	48.167130
1809.464075	190.252609	48.172135
1805.383418	186.493706	48.177140
1802.240056	191.108627	48.182145
1799.190454	193.128012	48.187149
1794.995643	191.573095	48.192154
1791.919056	190.462319	48.197159
1788.166066	188.320606	48.202164
1784.739865	197.084738	48.207169
1781.519188	185.185767	48.212173
1777.713049	191.191010	48.217178
1774.368207	195.244484	48.222183
1770.865671	188.061935	48.227188
1767.176718	192.596412	48.232193
1763.678037	192.912709	48.237197
1760.204817	193.199551	48.242202
1756.956123	190.538879	48.247207
1752.946903	187.467302	48.252212
1749.635540	193.758712	48.257217
1746.639295	187.106282	48.262221
1742.466679	195.411910	48.267226
1739.019352	183.344466	48.272231
1735.472313	186.107644	48.277236
1732.136441	186.796454	48.282241
1728.827205	182.359809	48.287245
1725.184442	194.247250	48.292250
1721.797230	184.110175	48.297255
1718.057156	189.017942	48.302260
1714.843844	201.847930	48.307265
1711.371619	186.819682	48.312269
1707.574064	185.226301	48.317274
1703.994902	193.182252	48.322279
1700.814129	178.247007	48.327284
1697.249843	181.928382	48.332289
1693.904364	178.070930	48.337293
1690.019792	197.529819	48.342298
1686.406665	176.746535	48.347303
1683.302555	199.077378	48.352308
1679.483505	189.891006	48.357313
1676.430337	199.409318	48.362317
1672.615450	188.703349	48.367322
1669.063569	180.003281	48.372327
1665.482593	196.748851	48.377332
1662.158769	190.190373	48.382337
1658.735025	186.942230	48.387341
1655.101520	190.436847	48.392346
1651.794105	177.642855	48.397351
1648.431114	187.569431	48.402356
1644.693382	180.635708	48.407361
1641.211498	179.708393	48.412365
1637.645838	191.651708	48.417370
1634.313769	183.645740	48.422375
1630.875496	175.080263	48.427380
1627.101643	178.453224	48.432385
1623.475690	176.341250	48.437389
1619.997560	183.611176	48.442394
1616.648443	166.181032	48.447399
1613.039780	180.953804	48.452404
1609.525171	177.857322	48.457409
1606.511329	179.881340	48.462413
1602.413457	185.850553	48.467418
1599.100420	186.168556	48.472423
1595.422974	186.153353	48.477428
1591.992900	183.821623	48.482433
1588.726886	176.629649	48.487437
1584.681400	189.886849	48.492442
1581.541759	180.914980	48.497447
1578.284524	181.295803	48.502452
1574.372979	181.995532	48.507457
1571.186379	177.972621	48.512461
1567.540757	181.875051	48.517466
1564.552586	183.239575	48.522471
1560.967215	188.571561	48.527476
1557.067148	177.565611	48.532481
1553.663082	188.805210	48.537485
1549.916374	184.681671	48.542490
1546.868148	174.075986	48.547495
1543.173957	178.907694	48.552500
1539.433742	172.169098	48.557505
1536.042749	183.536670	48.562509
1532.410134	178.916423	48.567514
1529.260503	166.749185	48.572519
1525.487913	170.868419	48.577524
1521.951630	171.878969	48.582529
1519.073513	172.100274	48.587533
1514.898752	167.689774	48.592538
1511.445634	179.669309	48.597543
1507.843180	171.907721	48.602548
1504.222844	183.605571	48.607553
1501.223329	170.348972	48.612557
1497.537973	170.978956	48.617562
1493.887410	171.860890	48.622567
1490.441663	169.485433	48.627572
1487.071430	170.271778	48.632577
1483.631872	174.761969	48.637581
1479.773492	170.169445	48.642586
1476.799345	171.335562	48.647591
1473.081650	177.613831	48.652596
1469.543877	176.440800	48.657601
1466.349858	160.301535	48.662605
1462.182242	178.946714	48.667610
1458.916671	164.600593	48.672615
1455.256879	160.043286	48.677620
1451.914795	178.219257	48.682625
1448.828923	167.575053	48.687629
1444.896073	175.953322	48.692634
1441.538091	173.806494	48.697639
1438.334670	165.609921	48.702644
1434.281360	171.434927	48.707649
1430.923440	158.086687	48.712653
1427.499454	169.247623	48.717658
1424.176385	163.051525	48.722663
1420.614606	165.362082	48.727668
1417.065760	174.377147	48.732673
1413.481201	163.902583	48.737677
1409.850187	162.629349	48.742682
1406.543197	159.199292	48.747687
1402.983222	172.679988	48.752692
1399.033552	165.316041	48.757697
1395.738194	151.974866	48.762701
1392.468774	164.217812	48.767706
1389.040810	159.739286	48.772711
1385.822194	167.916231	48.777716
1381.823223	170.507131	48.782721
1378.657572	164.060435	48.787725
1374.658371	165.023355	48.792730
1371.329530	164.813699	48.797735
1368.048688	165.459065	48.802740
1364.403327	167.524375	48.807745
1360.866459	162.636066	48.812749
1357.475152	164.800523	48.817754
1353.955173	166.758622	48.822759
1350.531968	162.662904	48.827764
1346.552180	165.326917	48.832769
1343.360008	164.794210	48.837773
1339.652994	160.202539	48.842778
1336.770812	154.895912	48.847783
1333.158863	165.862181	48.852788
1329.346007	169.173951	48.857793
1326.206329	162.470240	48.862797
1322.347017	171.949956	48.867802
1318.960490	158.180610	48.872807
1315.350534	164.933655	48.877812
1311.660267	160.488897	48.882817
1308.229805	163.007208	48.887821
1305.047733	161.530293	48.892826
1301.681697	164.407538	48.897831
1298.129726	160.104617	48.902836
1294.182293	156.291986	48.907841
1290.998739	157.919529	48.912845
1287.413640	169.456156	48.917850
1283.426816	149.736645	48.922855
1280.200643	163.715047	48.927860
1276.648231	160.521399	48.932865
1273.505960	164.575582	48.937869
1269.873316	160.414246	48.942874
1266.622066	159.927139	48.947879
1262.824330	160.984330	48.952884
1259.294025	165.240592	48.957889
1255.932685	157.989171	48.962893
1252.058585	169.202177	48.967898
1248.698653	165.338269	48.972903
1245.374228	172.912782	48.977908
1241.843587	168.454143	48.982913
1238.460208	148.631011	48.987917
1234.765644	170.439518	48.992922
1231.158675	156.099096	48.997927
1227.862959	160.681771	49.002932
1224.011013	171.045062	49.007937
1221.276604	156.471226	49.012941
1217.454009	160.496067	49.017946
1213.761875	155.766363	49.022951
1210.431919	164.246867	49.027956
1206.635258	161.690346	49.032961
1203.611898	156.163111	49.037965
1199.866209	166.113653	49.042970
1196.301670	162.932015	49.047975
1192.602236	160.503194	49.052980
1188.888677	166.473202	49.057985
1185.767520	168.147713	49.062989
1182.154561	161.802391	49.067994
1178.477902	156.057254	49.072999
1174.788400	157.249344	49.078004
1171.612370	156.957930	49.083009
1168.780378	159.775586	49.088013
1165.112147	158.659966	49.093018
1161.432246	162.140180	49.098023
1157.739258	160.130588	49.103028
1154.061361	159.195334	49.108033
1150.685979	158.585329	49.113037
1147.217544	165.711683	49.118042
1143.663898	157.109118	49.123047
1140.255471	164.537517	49.128052
1136.727817	157.723338	49.133057
1133.545293	155.982084	49.138061
1129.566697	160.130886	49.143066
1126.035298	147.162011	49.148071
1122.821355	166.920063	49.153076
1118.964065	164.816763	49.158081
1115.436035	156.393584	49.163085
1112.749165	160.417243	49.168090
1108.845563	157.122141	49.173095
1105.427688	157.904103	49.178100
1101.510884	167.451517	49.183105
1098.473004	153.389070	49.188109
1094.821896	168.902726	49.193114
1091.098688	165.851521	49.198119
1087.607039	158.812509	49.203124
1083.909617	166.556692	49.208129
1080.724932	155.518215	49.213133
1076.968103	164.194441	49.218138
1073.510972	154.910257	49.223143
1070.235864	160.654030	49.228148
1066.597671	167.366962	49.233153
1063.080834	156.907589	49.238157
1060.000591	159.602207	49.243162
1056.086260	156.375304	49.248167
1052.676000	150.769269	49.253172
1048.984466	162.431291	49.258177
1045.695009	156.092625	49.263181
1042.102209	158.324829	49.268186
1038.658178	158.447979	49.273191
1035.145377	156.063216	49.278196
1031.420818	159.440965	49.283201
1028.081248	157.785674	49.288205
1024.798389	154.823702	49.293210
1020.889966	150.572886	49.298215
1017.698581	158.714197	49.303220
1013.957644	161.968380	49.308225
1011.166268	151.180610	49.313229
1007.287735	152.917303	49.318234
1003.680920	164.611232	49.323239
1000.170669	152.975925	49.328244
996.674594	147.869279	49.333249
993.098495	161.192860	49.338253
989.348512	156.100712	49.343258
985.813458	160.926931	49.348263
982.865910	156.515712	49.353268
979.320487	171.538023	49.358273
975.566929	165.308280	49.363277
971.730481	158.001987	49.368282
968.508314	163.709538	49.373287
965.017914	159.871568	49.378292
961.607845	153.729260	49.383297
957.964294	151.983022	49.388301
954.534157	155.148823	49.393306
951.071708	170.313911	49.398311
947.633508	155.992481	49.403316
943.995899	159.182877	49.408321
940.480065	159.968467	49.413325
937.198484	154.227993	49.418330
933.752615	155.071586	49.423335
929.726687	151.523814	49.428340
926.176104	157.079812	49.433345
922.918944	153.561179	49.438349
919.490793	152.011827	49.443354
916.083327	148.397953	49.448359
912.787430	159.648027	49.453364
909.107436	164.809178	49.458369
905.634542	152.615884	49.463373
902.341700	156.799066	49.468378
898.609709	149.938467	49.473383
894.997819	153.133618	49.478388
891.143259	155.742379	49.483393
888.297214	152.048345	49.488397
884.451758	156.594481	49.493402
880.869422	153.779210	49.498407
877.429263	157.434555	49.503412
874.074549	153.705839	49.508417
870.328815	154.831214	49.513421
867.062501	153.001524	49.518426
863.583195	152.902004	49.523431
860.054481	155.212409	49.528436
855.999929	163.026027	49.533441
852.839250	145.439915	49.538445
849.145803	156.401880	49.543450
846.066216	159.545561	49.548455
842.604662	160.811668	49.553460
838.844152	156.253498	49.558465
835.681288	150.559577	49.563469
832.058790	155.466307	49.568474
828.376917	154.689641	49.573479
825.096698	154.538915	49.578484
821.130782	152.014421	49.583489
817.859259	154.475346	49.588493
814.468282	159.049762	49.593498
810.885216	157.564722	49.598503
807.442472	155.473558	49.603508
803.606813	156.997195	49.608513
800.293169	155.978309	49.613517
796.898213	151.030489	49.618522
793.514661	156.692250	49.623527
790.279574	152.268924	49.628532
786.733692	150.444993	49.633537
782.941329	146.322751	49.638541
778.829362	151.052551	49.643546
775.944922	149.169611	49.648551
772.604765	152.652221	49.653556
768.832767	151.541824	49.658561
765.644867	141.519239	49.663565
761.746135	152.616558	49.668570
758.030373	155.305269	49.673575
754.851643	139.394616	49.678580
751.197544	149.891177	49.683585
748.053628	151.116516	49.688589
744.093451	151.038167	49.693594
740.722339	155.446456	49.698599
737.344831	149.731013	49.703604
733.873801	148.677185	49.708609
730.584769	149.773286	49.713613
726.965558	152.971211	49.718618
723.373318	157.968398	49.723623
720.116065	151.031680	49.728628
716.151206	149.045735	49.733633
712.854200	134.467254	49.738637
709.081468	152.788330	49.743642
705.948002	149.758642	49.748647
702.462898	154.594108	49.753652
698.849016	151.077582	49.758657
695.098481	156.290738	49.763661
691.815295	144.811403	49.768666
688.324050	154.882828	49.773671
685.116444	145.149051	49.778676
681.433270	141.371299	49.783681
678.033634	149.723131	49.788685
674.468551	152.974000	49.793690
670.708755	150.854179	49.798695
666.838556	147.110085	49.803700
663.278497	151.118590	49.808705
660.198306	143.890047	49.813709
657.015530	149.001854	49.818714
653.250904	140.965904	49.823719
650.074976	135.571297	49.828724
646.302582	156.383976	49.833729
643.066111	149.824285	49.838733
638.528208	158.001085	49.843738
635.237438	144.537504	49.848743
632.395256	150.571234	49.853748
628.936148	149.206407	49.858753
625.792244	143.141585	49.863757
622.089972	147.563779	49.868762
618.378640	147.217203	49.873767
614.934673	144.193564	49.878772
610.997285	153.134623	49.883777
607.502453	133.367171	49.888781
603.884682	143.367083	49.893786
600.528524	138.666218	49.898791
597.300720	129.084414	49.903796
593.574370	144.909392	49.908801
590.159953	135.720474	49.913805
586.670592	143.114226	49.918810
582.891978	141.401264	49.923815
579.916430	137.249503	49.928820
576.505733	148.016601	49.933825
572.540257	136.652409	49.938829
569.172430	147.657489	49.943834
565.977478	152.870791	49.948839
562.512605	130.149531	49.953844
558.553762	138.574537	49.958849
555.248565	139.473322	49.963853
551.884363	131.695781	49.968858
547.865049	154.791606	49.973863
544.601063	138.630185	49.978868
541.186055	142.858370	49.983873
537.986441	137.464381	49.988877
534.102615	127.866176	49.993882
530.254767	144.403113	49.998887
526.987870	139.570343	50.003892
523.668925	142.960479	50.008897
520.151107	137.584136	50.013901
517.171276	139.459746	50.018906
513.158126	140.793554	50.023911
509.610271	132.817593	50.028916
505.618866	148.617530	50.033921
502.583453	137.099760	50.038925
499.386306	143.155766	50.043930
495.370232	140.399836	50.048935
492.595993	131.607585	50.053940
488.677127	141.036942	50.058945
484.952812	135.320632	50.063949
481.565172	137.695630	50.068954
477.786608	144.975115	50.073959
474.872907	136.582967	50.078964
471.037017	137.944246	50.083969
467.830994	134.757377	50.088973
464.207090	139.034508	50.093978
460.695795	141.954689	50.098983
457.338811	127.456238	50.103988
453.591264	133.589566	50.108993
449.437524	131.805862	50.113997
446.480436	130.876935	50.119002
442.947287	134.428572	50.124007
439.598769	129.747849	50.129012
436.185533	136.176383	50.134017
433.082066	129.264257	50.139021
429.214037	129.262429	50.144026
425.126292	125.512207	50.149031
421.974305	116.276010	50.154036
418.358344	135.614355	50.159041
414.769021	129.933604	50.164045
411.885739	134.280396	50.169050
407.874435	129.770444	50.174055
404.484957	123.426186	50.179060
400.501679	131.684437	50.184065
397.392177	129.596953	50.189069
393.972417	129.540035	50.194074
390.589771	138.578678	50.199079
387.565744	132.737767	50.204084
383.546458	143.739058	50.209089
380.058177	137.339310	50.214093
376.423501	135.075285	50.219098
372.708380	135.428643	50.224103
369.303207	129.711382	50.229108
365.927711	130.890314	50.234113
362.531033	140.387368	50.239117
359.191428	134.174095	50.244122
355.571478	143.430424	50.249127
352.188809	132.970573	50.254132
348.676000	133.930988	50.259137
345.252185	131.062219	50.264141
341.636728	132.189057	50.269146
337.591564	130.342504	50.274151
334.384587	134.108750	50.279156
330.786011	136.919900	50.284161
327.140901	134.412373	50.289165
324.134777	129.403257	50.294170
320.414662	143.512104	50.299175
316.904840	129.070764	50.304180
313.010699	130.917767	50.309185
310.099057	138.352441	50.314189
306.472827	131.609226	50.319194
302.723273	132.750052	50.324199
299.524914	128.124808	50.329204
295.961408	129.034829	50.334209
292.510866	142.299357	50.339213
289.144933	135.266016	50.344218
285.151070	134.596060	50.349223
282.083512	134.567434	50.354228
278.544844	139.873063	50.359233
275.094543	135.680323	50.364237
271.345428	139.434851	50.369242
267.716646	146.282352	50.374247
264.333078	139.799866	50.379252
261.159822	144.501447	50.384257
256.979778	138.972944	50.389261
253.703077	135.832691	50.394266
250.411382	137.249998	50.399271
247.257527	140.166478	50.404276
243.475539	132.674796	50.409281
239.483095	132.580777	50.414285
236.116978	128.361132	50.419290
233.044640	136.099801	50.424295
229.380727	142.159546	50.429300
225.922291	143.781797	50.434305
222.478225	140.869975	50.439309
219.344167	132.018441	50.444314
215.176395	143.379678	50.449319
211.810404	140.331546	50.454324
208.342004	135.814401	50.459329
204.556762	138.714470	50.464333
201.496924	132.850275	50.469338
197.819409	136.523856	50.474343
194.236390	127.929031	50.479348
190.742083	124.784815	50.484353
187.517708	142.085163	50.489357
183.861074	134.584449	50.494362
180.377193	136.292218	50.499367
176.743644	129.418889	50.504372
173.017947	136.153110	50.509377
169.572980	135.254120	50.514381
166.245943	130.079592	50.519386
163.026961	127.898937	50.524391
159.641006	130.563072	50.529396
155.952365	127.966259	50.534401
152.399126	128.551964	50.539405
148.731740	131.117486	50.544410
145.193146	125.585087	50.549415
141.978682	142.124370	50.554420
138.331544	131.630618	50.559425
134.825020	126.960788	50.564429
131.230576	134.155664	50.569434
127.771665	133.415171	50.574439
124.395554	119.177308	50.579444
120.726324	129.285673	50.584449
117.143593	127.661775	50.589453
114.129296	127.165193	50.594458
110.154626	134.303142	50.599463
106.466021	132.469543	50.604468
102.865987	127.114541	50.609473
99.671202	130.556576	50.614477
96.585992	121.178719	50.619482
92.741049	139.561672	50.624487
89.290864	136.218339	50.629492
85.617799	126.079529	50.634497
82.268267	125.629184	50.639501
78.418010	123.435098	50.644506
75.337650	132.566279	50.649511
72.011663	121.861959	50.654516
68.152228	126.085479	50.659521
64.710175	126.371497	50.664525
61.346310	128.424420	50.669530
57.312425	128.447956	50.674535
54.176565	128.355158	50.679540
50.763947	139.812677	50.684545
47.149420	140.283672	50.689549
43.699567	126.000430	50.694554
39.950857	136.961620	50.699559
37.004384	125.969868	50.704564
33.423803	121.831164	50.709569
29.731343	133.308394	50.714573
26.421196	132.898727	50.719578
22.696927	131.071270	50.724583
19.123134	129.576669	50.729588
15.510482	133.981608	50.734593
11.926435	139.457353	50.739597
8.605913	131.145322	50.744602
4.690805	128.351032	50.749607
1.594002	125.555782	50.754612