Thu Jun 16 10:55:12 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
1.137745	115.697069	0.000000
1.122970	111.758263	0.005005
0.785387	95.507410	0.010010
1.044212	91.455717	0.015014
0.430556	85.779840	0.020019
0.390649	70.354091	0.025024
0.161114	65.153983	0.030029
-0.049818	55.432659	0.035034
-0.298250	45.290663	0.040038
-1.073030	34.324297	0.045043
-1.144368	33.104478	0.050048
-1.257756	31.482197	0.055053
-1.643656	15.538137	0.060058
-2.311952	10.003909	0.065062
-2.544414	10.205186	0.070067
-2.171303	8.222233	0.075072
-2.916524	4.285587	0.080077
-3.662076	1.175909	0.085082
-3.494884	0.529508	0.090086
-3.670316	5.298581	0.095091
-4.236780	3.931023	0.100096
-4.198212	1.990039	0.105101
-4.928940	-0.707447	0.110106
-5.279528	1.485925	0.115110
-5.574366	11.143870	0.120115
-5.430662	8.189999	0.125120
-5.772952	5.646933	0.130125
-5.759278	5.129587	0.135130
-5.461098	9.224328	0.140134
-5.480664	5.190548	0.145139
-6.362560	9.785643	0.150144
-6.752722	2.236824	0.155149
-7.291993	6.049699	0.160154
-7.129526	4.241645	0.165158
-8.022556	7.814063	0.170163
-8.526197	3.692967	0.175168
-8.407035	0.508753	0.180173
-8.577501	12.149992	0.185178
-8.818629	8.867078	0.190182
-8.685070	12.165861	0.195187
-8.874803	1.839677	0.200192
-8.586552	4.982671	0.205197
-9.452072	5.414154	0.210202
-10.160961	-4.438225	0.215206
-10.334964	9.367557	0.220211
-10.560965	6.350383	0.225216
-10.337877	-2.574678	0.230221
-10.309255	13.268651	0.235226
-10.680932	6.184591	0.240230
-11.158095	14.877454	0.245235
-11.499056	11.616957	0.250240
-11.567205	8.771003	0.255245
-12.339952	9.192186	0.260250
-12.745592	-0.464072	0.265254
-13.326590	9.523903	0.270259
-13.340475	6.316493	0.275264
-13.077934	-0.039940	0.280269
-13.391834	7.343543	0.285274
-13.326259	5.408849	0.290278
-13.527757	7.319901	0.295283
-13.557001	5.959551	0.300288
-14.095240	6.323235	0.305293
-14.623698	9.935735	0.310298
-15.071686	-0.619064	0.315302
-14.911642	7.629910	0.320307
-15.356996	11.151727	0.325312
-15.914743	-2.404515	0.330317
-16.548025	16.633687	0.335322
-16.490067	13.767778	0.340326
-16.806546	3.965081	0.345331
-16.378242	9.596053	0.350336
-16.613362	10.655857	0.355341
-16.934727	10.335547	0.360346
-16.683396	7.527260	0.365350
-17.300333	15.874061	0.370355
-17.907248	14.314600	0.375360
-17.773264	3.370916	0.380365
-18.388354	12.920686	0.385370
-18.445491	6.183007	0.390374
-19.001093	7.458652	0.395379
-19.633351	8.976630	0.400384
-19.493806	6.870880	0.405389
-19.821292	6.880886	0.410394
-19.737905	9.926725	0.415398
-20.087823	11.152002	0.420403
-20.019550	11.040273	0.425408
-20.245458	12.857791	0.430413
-21.469526	20.115763	0.435418
-21.287642	5.175701	0.440422
-21.330320	8.505384	0.445427
-21.488182	11.141530	0.450432
-21.329672	8.275085	0.455437
-22.142665	19.384128	0.460442
-22.524780	11.368925	0.465446
-23.086733	20.687652	0.470451
-23.042536	-1.458678	0.475456
-22.615768	4.876437	0.480461
-23.194392	13.557852	0.485466
-23.341514	-9.350121	0.490470
-24.217673	9.873922	0.495475
-24.516781	4.628806	0.500480
-24.413454	-0.318390	0.505485
-24.615110	6.009498	0.510490
-24.507123	7.109082	0.515494
-24.898495	17.922726	0.520499
-25.551011	11.320633	0.525504
-25.643818	-3.714308	0.530509
-26.166108	16.504878	0.535514
-25.856730	-1.376586	0.540518
-26.138236	6.678501	0.545523
-27.012630	3.746386	0.550528
-27.157160	5.054130	0.555533
-28.021800	18.044346	0.560538
-27.374497	4.187238	0.565542
-27.173608	8.402134	0.570547
-27.813662	-3.640772	0.575552
-27.875809	-8.538027	0.580557
-28.468877	5.429444	0.585562
-28.311834	0.620463	0.590566
-28.938636	0.158257	0.595571
-29.254325	0.545736	0.600576
-29.318730	4.506147	0.605581
-29.781449	8.659058	0.610586
-29.481429	-1.129010	0.615590
-30.142401	13.420203	0.620595
-30.538564	9.772146	0.625600
-30.578165	3.328124	0.630605
-30.952493	18.073445	0.635610
-30.973055	-3.470158	0.640614
-31.234898	1.661835	0.645619
-31.962804	9.573364	0.650624
-32.208431	-9.223421	0.655629
-32.584083	4.975074	0.660634
-32.671408	-1.095351	0.665638
-32.777482	-1.457455	0.670643
-32.892972	-2.900329	0.675648
-32.738143	-5.958833	0.680653
-32.877754	3.567992	0.685658
-33.564171	-5.653557	0.690662
-34.077416	8.250609	0.695667
-34.199730	9.156122	0.700672
-34.186475	1.597757	0.705677
-34.464970	8.948456	0.710682
-34.749780	6.685539	0.715686
-35.460325	-2.733473	0.720691
-35.712855	4.284516	0.725696
-35.491061	-5.287099	0.730701
-35.675088	1.204103	0.735706
-35.726766	-2.605356	0.740710
-36.465279	0.944191	0.745715
-36.757558	7.765821	0.750720
-36.874706	3.724296	0.755725
-37.325614	3.439405	0.760730
-37.488537	13.446189	0.765734
-37.392711	14.736309	0.770739
-38.072817	11.326961	0.775744
-38.428031	10.883109	0.780749
-38.944096	6.702016	0.785754
-38.722413	-0.788885	0.790758
-38.722441	5.702888	0.795763
-38.847737	3.459780	0.800768
-39.193826	4.857955	0.805773
-39.490779	3.422281	0.810778
-39.924473	8.716550	0.815782
-40.489577	4.034807	0.820787
-40.686055	6.700715	0.825792
-40.238084	2.582171	0.830797
-40.536268	8.128696	0.835802
-41.062131	8.573896	0.840806
-41.890024	2.119967	0.845811
-42.301189	5.258685	0.850816
-42.050296	0.498910	0.855821
-42.091130	9.674387	0.860826
-42.229791	0.510093	0.865830
-42.234590	11.354453	0.870835
-42.905784	7.259078	0.875840
-42.843418	3.295319	0.880845
-43.704988	6.320737	0.885850
-43.804916	-4.303415	0.890854
-43.916921	7.528816	0.895859
-43.984593	3.659552	0.900864
-44.241005	6.667136	0.905869
-44.880029	5.312166	0.910874
-44.934719	3.513167	0.915878
-45.346255	11.062542	0.920883
-45.450001	1.749233	0.925888
-45.368265	4.561732	0.930893
-45.645278	1.063079	0.935898
-46.513597	1.228271	0.940902
-47.059127	12.957340	0.945907
-47.124595	-0.643160	0.950912
-46.744654	14.530057	0.955917
-47.188619	0.569182	0.960922
-47.170834	7.565089	0.965926
-47.267486	8.924606	0.970931
-47.956987	7.342591	0.975936
-48.097521	0.703937	0.980941
-48.840604	6.464175	0.985946
-48.670668	0.633974	0.990950
-48.580859	2.080466	0.995955
-48.829827	6.287727	1.000960
-49.772939	8.231175	1.005965
-50.376309	13.945734	1.010970
-50.162440	5.484583	1.015974
-50.299548	1.969813	1.020979
-50.477548	7.985105	1.025984
-50.337749	15.845870	1.030989
-50.895425	4.757138	1.035994
-51.573261	11.417658	1.040998
-51.979005	9.894898	1.046003
-51.882202	6.176718	1.051008
-51.987798	1.591087	1.056013
-51.932373	12.615795	1.061018
-52.044046	3.491829	1.066022
-52.184068	1.837453	1.071027
-52.795739	8.314294	1.076032
-53.056903	8.952517	1.081037
-53.849094	7.954140	1.086042
-53.679367	15.538661	1.091046
-53.802934	2.701374	1.096051
-54.272899	7.382983	1.101056
-54.679968	2.443584	1.106061
-54.972289	-0.214576	1.111066
-55.320510	10.217639	1.116070
-55.038235	11.266615	1.121075
-55.536153	3.324523	1.126080
-55.246609	0.711075	1.131085
-55.541563	5.879223	1.136090
-56.429372	6.241195	1.141094
-56.953712	15.322558	1.146099
-56.625803	10.839106	1.151104
-56.716713	8.621489	1.156109
-57.123330	10.998347	1.161114
-56.795482	14.597479	1.166118
-57.794416	3.688123	1.171123
-58.580238	7.777628	1.176128
-58.449513	5.402630	1.181133
-58.659717	-1.471930	1.186138
-58.907565	9.372344	1.191142
-58.794117	9.198396	1.196147
-58.661803	5.374707	1.201152
-59.479775	9.273206	1.206157
-59.919299	3.020078	1.211162
-60.086697	4.494873	1.216166
-60.205251	13.798224	1.221171
-60.418537	1.686960	1.226176
-60.365844	3.101111	1.231181
-61.213790	4.158316	1.236186
-61.324447	9.169729	1.241190
-61.806753	2.853727	1.246195
-62.297756	4.602198	1.251200
-61.882939	1.722695	1.256205
-62.134004	17.128250	1.261210
-61.989373	7.743899	1.266214
-62.294012	8.424625	1.271219
-63.080474	8.401872	1.276224
-62.875453	11.085871	1.281229
-63.356863	11.729912	1.286234
-63.235657	4.912154	1.291238
-64.278172	6.389025	1.296243
-64.860481	7.761230	1.301248
-64.858575	0.774072	1.306253
-65.075019	6.244934	1.311258
-64.903652	12.286540	1.316262
-64.743097	3.705558	1.321267
-64.968069	7.072667	1.326272
-65.295363	4.687440	1.331277
-66.161577	13.324440	1.336282
-66.511997	6.984864	1.341286
-66.818618	0.451597	1.346291
-67.068601	6.236689	1.351296
-66.625638	-0.627930	1.356301
-67.017823	6.449444	1.361306
-67.731188	5.665042	1.366310
-68.127851	19.850545	1.371315
-68.266159	12.102951	1.376320
-68.034216	1.476236	1.381325
-68.181438	4.038605	1.386330
-68.142716	0.725033	1.391334
-68.983377	1.353077	1.396339
-70.006549	17.048621	1.401344
-69.694804	-6.454098	1.406349
-70.055496	16.845558	1.411354
-70.035094	7.405580	1.416358
-69.900261	12.218675	1.421363
-70.089056	20.235360	1.426368
-70.828688	-1.141549	1.431373
-71.589952	8.662338	1.436378
-71.178456	6.943940	1.441382
-71.408927	11.304905	1.446387
-71.526799	5.520987	1.451392
-71.413469	8.390810	1.456397
-72.242722	8.699009	1.461402
-72.733457	-2.058647	1.466406
-72.699942	7.629077	1.471411
-73.006608	1.501579	1.476416
-72.799374	1.773729	1.481421
-73.811955	11.685744	1.486426
-74.029331	6.758798	1.491430
-74.310028	10.831611	1.496435
-74.467654	8.069899	1.501440
-74.320976	5.156380	1.506445
-74.591727	4.709817	1.511450
-74.678776	4.008556	1.516454
-74.671428	1.242269	1.521459
-75.541512	3.668694	1.526464
-75.496031	3.535673	1.531469
-76.246347	10.209159	1.536474
-75.844668	12.160513	1.541478
-76.933752	3.769095	1.546483
-77.382670	7.663030	1.551488
-77.252607	2.752456	1.556493
-77.395106	-0.230864	1.561498
-77.867185	12.228627	1.566502
-77.896199	-2.885808	1.571507
-77.851231	4.150293	1.576512
-77.766632	7.074289	1.581517
-77.999096	7.116934	1.586522
-78.591862	9.701443	1.591526
-79.181502	2.120590	1.596531
-79.444296	17.115217	1.601536
-79.276422	-0.658406	1.606541
-79.539233	10.528300	1.611546
-80.035960	6.005635	1.616550
-80.738900	9.327338	1.621555
-81.263845	11.447326	1.626560
-81.318036	-0.677599	1.631565
-81.253705	6.104130	1.636570
-81.298073	-1.725966	1.641574
-81.132836	6.227069	1.646579
-81.400517	10.733087	1.651584
-81.501564	-8.066175	1.656589
-82.212629	5.656306	1.661594
-82.375617	0.162588	1.666598
-82.900031	0.528234	1.671603
-83.070422	9.767244	1.676608
-82.921890	-1.077912	1.681613
-83.796317	10.229903	1.686618
-84.477675	3.567776	1.691622
-84.336826	4.999419	1.696627
-84.657377	3.003056	1.701632
-84.365332	-1.876674	1.706637
-84.793238	13.679346	1.711642
-84.463996	5.816798	1.716646
-84.474766	6.849489	1.721651
-85.554624	2.462565	1.726656
-85.942406	3.253022	1.731661
-86.163604	6.378004	1.736666
-85.597331	13.642654	1.741670
-86.374012	-2.632577	1.746675
-87.238151	2.383106	1.751680
-87.471506	3.474484	1.756685
-87.519298	2.113355	1.761690
-87.362721	13.270110	1.766694
-87.245427	4.364213	1.771699
-87.818165	13.088259	1.776704
-88.367268	10.615685	1.781709
-88.967702	12.408289	1.786714
-89.372711	12.465345	1.791718
-89.267908	7.461771	1.796723
-89.020903	4.973144	1.801728
-89.147582	2.646116	1.806733
-89.245186	8.679885	1.811738
-90.191125	12.052406	1.816742
-90.671072	5.804186	1.821747
-90.708257	9.786932	1.826752
-90.632186	-0.905273	1.831757
-90.995307	5.047188	1.836762
-90.810664	7.553228	1.841766
-91.597284	14.042118	1.846771
-92.333102	16.754647	1.851776
-92.391452	8.380416	1.856781
-92.426063	18.370136	1.861786
-92.459854	16.890773	1.866790
-92.399812	5.235693	1.871795
-92.608112	21.112254	1.876800
-93.268057	9.865221	1.881805
-93.829002	7.144322	1.886810
-94.070071	12.906337	1.891814
-93.691399	1.394228	1.896819
-93.940059	11.306559	1.901824
-94.671353	-10.397459	1.906829
-95.679567	5.879530	1.911834
-95.578102	-5.259032	1.916838
-95.379377	2.748742	1.921843
-95.846445	7.371569	1.926848
-95.613322	6.406470	1.931853
-95.691693	12.070664	1.936858
-95.909645	2.306744	1.941862
-96.077669	15.330989	1.946867
-96.748619	10.552307	1.951872
-96.913744	-1.268976	1.956877
-97.306263	18.243608	1.961882
-97.519160	6.896648	1.966886
-97.830369	2.927451	1.971891
-98.356489	9.784769	1.976896
-98.781257	6.257267	1.981901
-98.809771	8.290472	1.986906
-98.843429	8.209894	1.991910
-98.754342	5.275804	1.996915
-98.975372	5.400476	2.006912
-99.059878	2.665372	2.016909
-99.079543	6.965451	2.026906
-98.057995	11.911784	2.036902
-97.566377	4.104448	2.046899
-97.087444	9.758723	2.056896
-96.412827	7.568423	2.066893
-96.188549	7.383299	2.076890
-95.262067	1.511788	2.086886
-94.674741	1.187983	2.096883
-94.644330	0.656576	2.106880
-94.454627	5.498973	2.116877
-93.486272	9.800325	2.126874
-93.255978	7.864622	2.136870
-92.131914	6.983301	2.146867
-91.975405	12.522694	2.156864
-91.519485	9.546396	2.166861
-91.204317	10.864296	2.176858
-90.310016	-0.929020	2.186854
-89.747153	-0.164032	2.196851
-89.842249	0.017847	2.206848
-88.777276	2.936120	2.216845
-88.318721	0.140944	2.226842
-88.402336	7.248094	2.236838
-87.562909	9.493321	2.246835
-87.228314	2.508990	2.256832
-86.423424	3.328064	2.266829
-85.647190	9.488297	2.276826
-85.437882	-1.596708	2.286822
-85.297353	-0.958096	2.296819
-84.314986	6.833343	2.306816
-84.045613	9.072475	2.316813
-83.973737	3.002851	2.326810
-83.154212	4.393318	2.336806
-82.353889	-3.199714	2.346803
-81.456629	2.993411	2.356800
-81.561390	5.011768	2.366797
-81.200575	0.561791	2.376794
-80.790788	3.841523	2.386790
-79.849960	3.883159	2.396787
-79.540893	3.275717	2.406784
-78.516352	-0.936450	2.416781
-78.303457	5.600138	2.426778
-77.774366	1.587206	2.436774
-77.556675	3.738668	2.446771
-77.397633	-0.300179	2.456768
-76.689684	0.569837	2.466765
-75.683906	8.810167	2.476762
-75.306497	6.120811	2.486758
-74.982755	-1.986627	2.496755
-74.673013	-2.322092	2.506752
-74.007820	7.659904	2.516749
-73.278038	0.435470	2.526746
-73.114028	2.316356	2.536742
-72.279712	-4.862429	2.546739
-71.479116	3.849749	2.556736
-71.604398	1.104146	2.566733
-71.578181	5.973862	2.576730
-70.265856	4.909753	2.586726
-70.185926	0.087472	2.596723
-69.352791	6.561904	2.606720
-68.890136	4.994376	2.616717
-68.930280	-0.647885	2.626714
-67.664920	-4.135147	2.636710
-67.070462	5.523529	2.646707
-66.908977	1.317933	2.656704
-66.714863	9.126402	2.666701
-65.823820	8.862297	2.676698
-65.436870	1.991059	2.686694
-65.075862	5.300635	2.696691
-64.042174	4.005354	2.706688
-64.110420	2.210363	2.716685
-63.776499	5.917213	2.726682
-62.731748	3.874663	2.736678
-62.343605	2.247489	2.746675
-62.145387	5.125830	2.756672
-61.101777	5.786870	2.766669
-60.707882	6.013284	2.776666
-60.548204	1.994384	2.786662
-60.102603	-1.223549	2.796659
-59.215975	4.933999	2.806656
-58.858551	1.211749	2.816653
-58.905728	1.419639	2.826650
-57.856957	2.932838	2.836646
-57.584572	3.230700	2.846643
-56.693231	4.347486	2.856640
-56.185167	3.328782	2.866637
-56.296585	0.845023	2.876634
-55.374325	-2.143889	2.886630
-54.874324	-2.464074	2.896627
-54.809283	-2.160838	2.906624
-53.467919	4.665467	2.916621
-52.990045	-2.290682	2.926618
-53.081278	1.129295	2.936614
-52.812827	-0.441992	2.946611
-51.979722	-2.755927	2.956608
-51.348897	-4.743895	2.966605
-50.996080	1.258335	2.976602
-49.799886	0.981287	2.986598
-49.812332	-0.222938	2.996595
-49.838352	5.054976	3.006592
-48.880370	0.008950	3.016589
-48.070118	-1.100294	3.026586
-47.914286	-1.675544	3.036582
-47.590708	-4.814882	3.046579
-46.766247	4.245063	3.056576
-46.529123	5.660814	3.066573
-45.818996	-2.817390	3.076570
-44.818881	-3.164416	3.086566
-44.755777	-5.362552	3.096563
-44.673446	-7.404435	3.106560
-44.290985	-0.840356	3.116557
-43.426098	3.810547	3.126554
-42.910608	7.924542	3.136550
-41.902078	3.175491	3.146547
-41.537413	2.621587	3.156544
-41.453196	4.766859	3.166541
-41.407208	0.813322	3.176538
-40.500250	4.485479	3.186534
-40.061286	-4.282921	3.196531
-38.959777	-3.431912	3.206528
-38.573528	-1.628895	3.216525
-38.647890	3.587763	3.226522
-38.317198	-0.222378	3.236518
-37.163729	0.186649	3.246515
-37.089390	-1.905230	3.256512
-36.177362	-3.800342	3.266509
-35.770164	-1.875287	3.276506
-35.563488	5.041795	3.286502
-34.704223	-1.409008	3.296499
-33.874612	2.664334	3.306496
-33.504494	1.397180	3.316493
-33.675420	-1.541305	3.326490
-33.243337	-4.979554	3.336486
-32.423310	-3.821097	3.346483
-31.946349	1.578263	3.356480
-30.814292	3.601482	3.366477
-30.793505	4.222843	3.376474
-30.504674	-5.605988	3.386470
-30.203403	-8.671949	3.396467
-29.424784	-4.776282	3.406464
-28.883862	-3.436667	3.416461
-28.153233	-2.531870	3.426458
-27.548587	-2.497342	3.436454
-27.164945	2.175557	3.446451
-27.349220	-6.797640	3.456448
-26.488642	-0.288176	3.466445
-25.597128	-2.389852	3.476442
-25.756040	-4.654324	3.486438
-24.340832	-2.919021	3.496435
-24.220412	-0.389997	3.506432
-24.187171	-0.228785	3.516429
-23.510808	1.772299	3.526426
-22.879213	2.777476	3.536422
-22.255415	-0.407625	3.546419
-21.314913	-3.225252	3.556416
-21.229755	4.713293	3.566413
-20.809087	1.168371	3.576410
-20.714790	-4.740096	3.586406
-19.668142	-4.455902	3.596403
-19.179658	-4.296779	3.606400
-18.957946	-7.324403	3.616397
-18.088600	-7.314210	3.626394
-17.580103	-2.892398	3.636390
-17.360330	1.020804	3.646387
-16.938333	-3.881668	3.656384
-16.200374	-4.080609	3.666381
-16.075392	-1.570169	3.676378
-15.408986	8.041562	3.686374
-14.289524	-3.500772	3.696371
-14.128992	-0.266669	3.706368
-13.942352	-4.572633	3.716365
-13.573418	-3.502414	3.726362
-12.905147	-0.381856	3.736358
-12.655658	-4.343736	3.746355
-11.615704	-6.650610	3.756352
-11.216753	-8.950724	3.766349
-10.864531	-12.324950	3.776346
-9.944312	-9.609737	3.786342
-9.892881	-5.949991	3.796339
-9.496219	-6.696713	3.806336
-8.818903	-3.810276	3.816333
-8.173056	-5.265831	3.826330
-7.998900	-10.979019	3.836326
-7.008359	-0.648008	3.846323
-6.635068	-1.992931	3.856320
-6.335140	-10.325156	3.866317
-6.106351	-6.602460	3.876314
-5.061558	3.348968	3.886310
-4.759927	2.526134	3.896307
-4.519270	3.319584	3.906304
-3.817643	13.425473	3.916301
-3.509681	15.180684	3.926298
-2.892081	29.337402	3.936294
-2.475935	33.993385	3.946291
-2.274998	42.302306	3.956288
-1.699278	53.003188	3.966285
-1.567010	70.264006	3.976282
-0.975996	93.655692	3.986278
-0.360588	118.032816	3.996275
0.000000	120.743359	4.001280
0.502079	143.365144	4.006285
0.489062	140.439318	4.011290
0.859077	150.349241	4.016294
0.654591	151.327041	4.021299
0.501935	160.114536	4.026304
1.097716	146.613274	4.031309
0.495806	155.602077	4.036314
0.830786	153.839093	4.041318
0.678162	164.977519	4.046323
1.132755	178.487591	4.051328
1.173947	168.095014	4.056333
1.230159	181.312710	4.061338
1.142874	169.558229	4.066342
1.056670	159.522728	4.071347
1.041672	164.716089	4.076352
0.854131	153.929710	4.081357
0.932715	167.146064	4.086362
1.159423	180.576991	4.091366
1.346302	188.801208	4.096371
1.075231	178.901215	4.101376
1.171008	183.016824	4.106381
1.357348	182.783080	4.111386
1.363559	183.342395	4.116390
0.923582	166.024078	4.121395
1.006256	171.445568	4.126400
1.357722	185.317781	4.131405
1.295806	186.450094	4.136410
1.228249	182.217714	4.141414
1.058248	187.226466	4.146419
1.011256	186.211759	4.151424
1.342640	182.545136	4.156429
1.447467	187.338685	4.161434
1.303443	191.040214	4.166438
1.192520	194.635053	4.171443
1.088373	193.559451	4.176448
1.389816	197.524466	4.181453
1.179005	192.574960	4.186458
1.467445	196.095909	4.191462
1.245407	197.764334	4.196467
1.292984	187.611012	4.201472
1.549326	197.873599	4.206477
1.415061	209.493615	4.211482
1.386623	195.556420	4.216486
1.002165	195.008971	4.221491
1.229397	193.415717	4.226496
1.434224	187.077427	4.231501
1.299274	200.854435	4.236506
1.499730	191.385074	4.241510
1.630439	197.415917	4.246515
1.465758	193.562535	4.251520
1.417749	188.333176	4.256525
1.343343	199.914978	4.261530
1.588229	189.802151	4.266534
1.526204	195.416262	4.271539
1.244399	193.145912	4.276544
1.347545	207.201640	4.281549
1.337009	220.183863	4.286554
1.757365	222.892990	4.291558
1.720752	226.299063	4.296563
1.788859	238.922914	4.301568
1.914816	228.490244	4.306573
1.666806	216.426861	4.311578
1.398941	213.501209	4.316582
1.485386	219.124335	4.321587
1.821313	223.444340	4.326592
2.011563	229.599625	4.331597
1.505529	225.386719	4.336602
1.871962	224.896997	4.341606
1.670874	230.158820	4.346611
1.843103	225.564595	4.351616
1.739150	228.989689	4.356621
1.827550	223.497846	4.361626
1.756172	222.338100	4.366630
1.691732	222.337782	4.371635
1.918452	218.642769	4.376640
2.088701	224.244649	4.381645
1.972168	226.105381	4.386650
1.859676	215.768457	4.391654
1.868004	216.795145	4.396659
1.760028	217.043923	4.401664
1.718983	225.885917	4.406669
1.697316	223.914609	4.411674
2.253013	227.022232	4.416678
2.065157	227.744140	4.421683
1.836402	229.516378	4.426688
2.227830	227.132101	4.431693
1.682648	225.471156	4.436698
1.997774	231.250056	4.441702
1.904624	228.861511	4.446707
1.769347	233.539964	4.451712
1.809046	231.005257	4.456717
1.411573	236.745062	4.461722
2.089834	234.664396	4.466726
1.969332	238.541699	4.471731
1.985788	235.888994	4.476736
2.263356	235.098854	4.481741
2.129339	238.027555	4.486746
1.867542	238.059359	4.491750
1.978008	234.309662	4.496755
1.712469	234.093671	4.501760
2.040252	232.847340	4.506765
1.902024	229.686180	4.511770
2.247625	250.207970	4.516774
2.086039	263.250411	4.521779
1.976279	268.920581	4.526784
2.529455	268.015538	4.531789
2.472434	268.125967	4.536794
2.452112	258.359893	4.541798
2.060313	246.546465	4.546803
1.664256	245.184067	4.551808
2.066385	247.211743	4.556813
1.970031	261.508356	4.561818
2.300788	268.227139	4.566822
2.509629	265.722187	4.571827
2.443991	273.451299	4.576832
2.571408	267.202819	4.581837
2.255491	274.404842	4.586842
2.499827	269.123492	4.591846
2.634199	265.768207	4.596851
2.361805	276.577268	4.601856
2.507357	266.515335	4.606861
2.286672	271.248363	4.611866
2.278375	269.325548	4.616870
2.379004	273.444820	4.621875
2.171407	274.977287	4.626880
2.411481	264.162190	4.631885
2.236478	273.549319	4.636890
2.785881	270.687088	4.641894
2.861786	268.297038	4.646899
2.198993	269.273831	4.651904
2.549703	263.828993	4.656909
2.581081	264.308482	4.661914
2.830465	272.964982	4.666918
2.731571	274.321735	4.671923
2.434631	265.402154	4.676928
2.779317	265.887580	4.681933
2.325372	276.923264	4.686938
2.736090	266.737895	4.691942
2.731330	268.729524	4.696947
1.990314	277.902293	4.701952
2.476471	267.256661	4.706957
2.423943	262.158741	4.711962
2.456526	267.848007	4.716966
2.681357	269.416150	4.721971
2.560820	272.387123	4.726976
2.562461	260.682100	4.731981
2.432181	272.499111	4.736986
2.036454	280.068893	4.741990
2.899740	281.136314	4.746995
2.963297	290.421186	4.752000
2.989288	275.559205	4.757005
2.903762	297.274114	4.762010
2.888064	290.895472	4.767014
2.943315	294.536766	4.772019
2.521993	287.002229	4.777024
2.787095	290.070776	4.782029
2.557434	291.455456	4.787034
2.816605	288.160932	4.792038
2.663071	291.239864	4.797043
2.759662	297.960658	4.802048
2.926409	288.243856	4.807053
2.524320	301.133007	4.812058
2.622011	286.841430	4.817062
2.959445	289.681080	4.822067
2.824980	292.808163	4.827072
3.118816	288.956822	4.832077
2.756738	302.940650	4.837082
2.733843	288.438836	4.842086
2.965213	301.205247	4.847091
2.855460	303.185721	4.852096
2.943546	294.811788	4.857101
3.118839	314.517222	4.862106
3.080068	307.762465	4.867110
2.917292	307.097182	4.872115
3.053612	339.163899	4.877120
3.459191	318.700427	4.882125
3.126244	307.892982	4.887130
2.657294	296.413784	4.892134
2.839251	310.178275	4.897139
2.950954	321.503097	4.902144
3.282593	330.725538	4.907149
3.535151	321.943797	4.912154
3.295439	318.408023	4.917158
3.576925	319.838754	4.922163
3.302249	317.315045	4.927168
3.350867	307.504102	4.932173
3.295867	311.267109	4.937178
3.060122	302.202235	4.942182
3.099868	302.634567	4.947187
2.580425	303.543475	4.952192
3.055753	314.744370	4.957197
2.871724	322.458247	4.962202
3.349699	326.771085	4.967206
3.254190	321.398981	4.972211
2.965805	328.295877	4.977216
3.174815	323.296877	4.982221
3.186744	328.463054	4.987226
3.098741	315.715908	4.992230
3.226234	334.295223	4.997235
3.098012	336.757923	5.002240
3.672307	335.997073	5.007245
3.413182	342.369324	5.012250
3.752723	331.786057	5.017254
3.632680	326.651425	5.022259
3.480787	332.200822	5.027264
3.324450	320.020396	5.032269
2.929992	329.661362	5.037274
3.653609	340.573223	5.042278
3.557491	355.630519	5.047283
3.611634	355.356270	5.052288
3.559187	330.467016	5.057293
3.732618	342.281836	5.062298
3.508003	331.382479	5.067302
3.711505	328.494136	5.072307
3.645654	326.472798	5.077312
3.467267	325.477231	5.082317
3.436551	333.058045	5.087322
3.530853	337.171868	5.092326
3.729376	338.310479	5.097331
3.568066	352.850739	5.102336
3.843568	345.280927	5.107341
3.640323	347.570554	5.112346
3.303571	335.492738	5.117350
3.847420	350.483435	5.122355
3.507828	361.255516	5.127360
3.565191	345.868170	5.132365
3.425517	367.121145	5.137370
3.720039	355.195494	5.142374
4.032730	358.752527	5.147379
3.879199	367.743812	5.152384
3.782049	348.868078	5.157389
3.667674	360.089312	5.162394
3.884534	359.346194	5.167398
3.799158	355.091357	5.172403
3.795584	365.198022	5.177408
4.079345	354.068822	5.182413
3.743600	368.764302	5.187418
3.865377	368.185275	5.192422
4.103892	357.656077	5.197427
3.791419	370.027824	5.202432
4.088392	351.991923	5.207437
3.922641	368.144767	5.212442
4.038414	359.553719	5.217446
4.173014	367.525628	5.222451
3.895799	374.603606	5.227456
4.230207	358.049438	5.232461
4.068429	363.545430	5.237466
3.899183	336.866320	5.242470
3.811882	341.922522	5.247475
3.901142	353.996125	5.252480
4.061416	358.564410	5.257485
3.906948	361.938491	5.262490
3.622410	355.809060	5.267494
3.897847	361.927728	5.272499
3.745539	363.788864	5.277504
4.252513	357.585453	5.282509
4.069095	369.806831	5.287514
3.894657	355.951035	5.292518
4.155766	368.751064	5.297523
3.928645	365.964265	5.302528
4.028612	369.489073	5.307533
4.133215	361.673233	5.312538
3.805982	364.111605	5.317542
3.923343	367.024932	5.322547
3.949071	375.106883	5.327552
4.273019	391.029163	5.332557
4.064346	396.265362	5.337562
4.137082	391.484891	5.342566
4.533290	398.014051	5.347571
4.427622	392.843971	5.352576
4.597856	385.041838	5.357581
4.478746	382.809883	5.362586
4.304204	361.756271	5.367590
4.139706	365.776331	5.372595
3.924064	364.465399	5.377600
4.660587	378.692356	5.382605
4.405754	389.432297	5.387610
4.387314	376.494839	5.392614
4.583336	375.667756	5.397619
4.393039	372.888287	5.402624
4.311032	365.286684	5.407629
4.250552	381.669081	5.412634
4.516688	374.220570	5.417638
4.305518	385.159286	5.422643
4.474563	399.622896	5.427648
4.538571	392.076470	5.432653
4.412979	390.872593	5.437658
4.596744	393.906261	5.442662
4.469611	402.392131	5.447667
4.357872	403.862598	5.452672
4.485321	398.366410	5.457677
4.281575	398.537689	5.462682
4.522905	405.488945	5.467686
4.413903	392.900095	5.472691
4.360867	391.768874	5.477696
4.320967	398.714217	5.482701
4.379904	402.688286	5.487706
4.539457	396.838340	5.492710
4.708456	400.179001	5.497715
4.553515	391.797725	5.502720
4.892139	396.197936	5.507725
4.381756	397.922321	5.512730
4.718097	402.103795	5.517734
4.503485	395.392067	5.522739
4.171724	403.570306	5.527744
4.522178	402.197782	5.532749
4.387829	418.737844	5.537754
4.964029	432.045431	5.542758
4.596773	426.688899	5.547763
4.678568	426.729034	5.552768
4.698709	422.810324	5.557773
4.813911	427.236614	5.562778
4.709866	431.599594	5.567782
4.942395	427.743552	5.572787
4.588624	442.727098	5.577792
4.776333	432.109858	5.582797
4.413769	433.395660	5.587802
4.618537	435.784700	5.592806
5.259605	431.074556	5.597811
4.888668	436.091240	5.602816
4.662709	428.823867	5.607821
4.800488	433.740103	5.612826
4.555933	430.985375	5.617830
4.745632	437.179311	5.622835
4.380976	433.160421	5.627840
5.039843	445.930296	5.632845
5.090584	455.129089	5.637850
5.179660	466.042710	5.642854
5.453858	458.052979	5.647859
4.967787	462.272219	5.652864
5.135104	429.947361	5.657869
5.049574	437.276142	5.662874
5.028326	434.669983	5.667878
5.081623	433.599026	5.672883
4.790839	442.845964	5.677888
5.125751	432.085714	5.682893
5.047098	456.176141	5.687898
5.459646	462.094807	5.692902
5.308598	441.738155	5.697907
5.052724	435.347350	5.702912
5.023191	442.095364	5.707917
5.297473	437.496346	5.712922
5.120343	424.199426	5.717926
5.249889	431.197087	5.722931
4.806855	438.003273	5.727936
5.647911	442.872842	5.732941
5.056323	442.755027	5.737946
5.237323	438.945875	5.742950
5.427276	435.323085	5.747955
4.899177	449.977031	5.752960
5.248814	448.084621	5.757965
5.189895	465.619549	5.762970
5.370764	461.210483	5.767974
5.705525	457.235726	5.772979
5.354320	466.570207	5.777984
5.726936	452.566994	5.782989
5.162077	450.324441	5.787994
5.139331	435.276895	5.792998
5.312353	437.640006	5.798003
5.430003	459.305092	5.803008
5.663170	451.925921	5.808013
5.381844	447.320359	5.813018
5.217271	450.974439	5.818022
5.265918	452.472272	5.823027
5.109196	456.381464	5.828032
5.482951	456.801715	5.833037
5.361755	455.171898	5.838042
5.575858	463.725715	5.843046
5.445423	460.264488	5.848051
5.329380	463.139453	5.853056
5.473575	466.809597	5.858061
5.295781	466.030473	5.863066
5.239719	457.970323	5.868070
5.493157	466.566773	5.873075
5.154423	469.957518	5.878080
5.391641	462.514829	5.883085
5.211612	475.356081	5.888090
5.328262	477.589705	5.893094
5.379746	482.942961	5.898099
5.360822	499.999247	5.903104
5.787244	490.175968	5.908109
5.763055	497.140266	5.913114
5.846680	493.929760	5.918118
5.854665	494.358270	5.923123
5.660193	499.982048	5.928128
5.796725	500.711132	5.933133
5.576303	499.923858	5.938138
6.161898	495.485388	5.943142
5.951261	499.857716	5.948147
5.746703	491.502047	5.953152
6.179250	490.466278	5.958157
5.882921	496.441531	5.963162
5.732161	495.953711	5.968166
5.719795	482.447984	5.973171
5.805666	497.097883	5.978176
6.111730	495.352465	5.983181
5.974639	480.071211	5.988186
6.057793	481.730173	5.993190
5.722538	471.854014	5.998195
5.661121	468.069526	6.003200
5.945388	482.560444	6.008205
5.900568	481.771775	6.013210
5.440450	497.510604	6.018214
5.549252	490.849173	6.023219
5.680996	504.430448	6.028224
6.075337	496.205672	6.033229
5.981870	496.211828	6.038234
5.899574	495.762712	6.043238
5.754567	487.837606	6.048243
6.244952	494.786221	6.053248
6.318223	488.554196	6.058253
6.048048	485.920205	6.063258
5.809657	482.617498	6.068262
6.019457	474.828117	6.073267
5.927761	486.542430	6.078272
5.601763	477.350598	6.083277
5.899251	485.878907	6.088282
6.328299	494.623637	6.093286
5.873188	470.796933	6.098291
5.424308	477.503374	6.103296
5.696687	477.387608	6.108301
5.710031	490.962194	6.113306
5.867227	496.519864	6.118310
6.063044	482.413839	6.123315
6.148131	498.413687	6.128320
6.454356	501.540496	6.133325
6.184116	482.215705	6.138330
5.922989	474.828236	6.143334
6.090201	458.653004	6.148339
6.013175	465.569095	6.153344
5.820355	465.810885	6.158349
6.211657	465.549579	6.163354
6.146909	466.651599	6.168358
6.131454	464.701628	6.173363
6.095560	472.772407	6.178368
6.043633	465.323141	6.183373
5.772171	471.195716	6.188378
5.964136	462.446501	6.193382
6.197934	466.744189	6.198387
5.936330	474.788043	6.203392
6.152334	468.469989	6.208397
5.982455	466.411365	6.213402
5.700352	454.349779	6.218406
5.685442	465.324585	6.223411
5.985673	464.580609	6.228416
5.880951	468.849100	6.233421
5.826397	471.934994	6.238426
5.802020	456.800089	6.243430
6.193810	469.870728	6.248435
5.863459	465.194633	6.253440
6.198115	455.463394	6.258445
5.978971	463.772517	6.263450
5.526953	448.051637	6.268454
5.620892	454.316258	6.273459
5.685878	467.833159	6.278464
6.127416	465.486934	6.283469
5.610304	464.129821	6.288474
5.842063	461.921952	6.293478
5.978935	460.857702	6.298483
5.959803	479.347674	6.303488
5.857734	468.884648	6.308493
6.084969	468.415260	6.313498
5.750828	466.124513	6.318502
6.014954	465.242564	6.323507
6.154491	468.775063	6.328512
6.082330	461.443584	6.333517
5.807283	465.072515	6.338522
6.163351	459.355122	6.343526
5.884377	448.946207	6.348531
5.392883	452.586439	6.353536
5.689675	455.773498	6.358541
5.916396	467.914940	6.363546
5.778182	470.643317	6.368550
5.954575	464.543330	6.373555
5.598704	464.956695	6.378560
5.554325	463.979126	6.383565
5.542094	469.775219	6.388570
5.567473	464.954900	6.393574
5.581785	464.911871	6.398579
5.704817	463.071707	6.403584
5.672041	467.537460	6.408589
5.934195	476.038849	6.413594
6.140054	472.462257	6.418598
6.266840	476.447429	6.423603
5.862975	470.271769	6.428608
5.871580	463.205252	6.433613
5.703894	472.374249	6.438618
5.519422	471.800645	6.443622
6.073507	466.815802	6.448627
5.972079	476.805427	6.453632
5.971253	458.925262	6.458637
6.079570	466.430088	6.463642
5.651328	463.453052	6.468646
5.957344	458.420712	6.473651
5.790427	461.947719	6.478656
5.846106	459.986684	6.483661
5.929765	462.959366	6.488666
5.671166	474.285909	6.493670
6.163519	473.294618	6.498675
5.929646	478.175505	6.503680
5.877088	468.964930	6.508685
5.706795	470.092087	6.513690
5.604200	465.381215	6.518694
6.075498	479.982595	6.523699
5.787477	490.317187	6.528704
6.057498	487.698697	6.533709
6.011145	472.283673	6.538714
5.706960	463.619016	6.543718
5.900069	464.648431	6.548723
5.760151	474.757377	6.553728
6.172142	475.285850	6.558733
6.151304	476.695427	6.563738
5.938012	466.222963	6.568742
5.915440	466.100988	6.573747
5.777086	465.843750	6.578752
6.055161	443.667002	6.583757
5.968619	458.444408	6.588762
5.429736	464.493177	6.593766
6.113394	461.131623	6.598771
5.954582	462.451236	6.603776
6.087129	464.102822	6.608781
6.055893	464.477830	6.613786
5.829669	470.081984	6.618790
5.975995	465.087378	6.623795
6.003459	466.701675	6.628800
5.914930	464.183188	6.633805
6.024544	467.484152	6.638810
5.970823	474.424414	6.643814
6.295118	452.890555	6.648819
6.024977	465.395277	6.653824
6.027502	451.391467	6.658829
6.072696	466.116033	6.663834
5.961648	460.621945	6.668838
6.343510	457.715941	6.673843
5.876746	469.612487	6.678848
5.969126	461.290930	6.683853
6.195949	464.643753	6.688858
6.004771	456.641647	6.693862
5.834698	439.367798	6.698867
5.488987	442.776561	6.703872
5.835397	446.733618	6.708877
5.400968	456.808845	6.713882
5.825913	451.620905	6.718886
6.009319	457.598846	6.723891
5.757643	463.872442	6.728896
5.835571	448.187205	6.733901
5.724769	457.990920	6.738906
6.030271	455.017427	6.743910
5.963287	460.147558	6.748915
5.815998	463.195995	6.753920
5.799585	457.579522	6.758925
5.914537	464.625190	6.763930
5.774706	458.290965	6.768934
6.047810	459.955628	6.773939
5.674559	462.079311	6.778944
5.765410	463.588126	6.783949
6.311688	459.719984	6.788954
5.950094	464.327387	6.793958
6.234361	457.073744	6.798963
5.916836	459.027407	6.803968
5.928061	461.262765	6.808973
6.039723	457.303370	6.813978
6.173649	460.382481	6.818982
6.034962	455.673038	6.823987
5.848593	436.868372	6.828992
5.733072	424.240814	6.833997
5.858022	445.557997	6.839002
6.003057	450.033822	6.844006
6.102718	444.590551	6.849011
5.935398	436.735061	6.854016
5.828406	426.055046	6.859021
5.979263	430.183817	6.864026
5.941363	429.782416	6.869030
6.125651	414.117520	6.874035
5.263921	427.090825	6.879040
5.391720	433.697506	6.884045
5.945757	438.378126	6.889050
6.088658	457.919507	6.894054
6.390530	452.611519	6.899059
6.012455	444.934991	6.904064
5.666980	433.115638	6.909069
5.690924	441.182726	6.914074
6.104997	449.910371	6.919078
6.241043	451.056454	6.924083
5.758946	434.062171	6.929088
6.000138	426.675964	6.934093
5.970780	425.643332	6.939098
5.606441	431.213766	6.944102
5.870763	429.233743	6.949107
6.107347	420.036284	6.954112
5.988696	431.337793	6.959117
6.071711	421.855932	6.964122
5.956016	416.207638	6.969126
6.062422	413.815485	6.974131
5.544329	420.661197	6.979136
5.904205	423.723581	6.984141
5.856958	421.334621	6.989146
5.703788	425.459571	6.994150
5.663769	421.392263	6.999155
5.702533	427.791679	7.004160
6.137215	443.826729	7.009165
6.076395	430.504959	7.014170
6.150612	429.235502	7.019174
6.254509	424.089381	7.024179
5.835380	425.533600	7.029184
6.113714	421.192099	7.034189
6.176566	430.107311	7.039194
6.014048	426.649124	7.044198
6.069583	421.707223	7.049203
5.688573	426.154548	7.054208
5.774212	427.565663	7.059213
5.906956	429.078107	7.064218
6.022113	420.942524	7.069222
5.997273	426.177259	7.074227
5.834094	423.880365	7.079232
6.229267	420.311567	7.084237
6.406843	428.086986	7.089242
5.976721	425.079586	7.094246
6.376190	411.644276	7.099251
5.596785	412.765444	7.104256
5.750860	406.261225	7.109261
5.888690	418.616802	7.114266
5.722600	424.087681	7.119270
5.861053	418.868863	7.124275
5.650874	430.702751	7.129280
5.996308	426.226545	7.134285
6.119447	418.148442	7.139290
5.634953	427.331588	7.144294
5.762261	415.974752	7.149299
5.562737	424.616141	7.154304
5.669431	415.072163	7.159309
6.200823	424.323309	7.164314
5.685831	429.827778	7.169318
6.152505	413.220517	7.174323
5.923415	431.640849	7.179328
5.814754	425.728865	7.184333
6.277570	426.320167	7.189338
5.787519	428.571077	7.194342
6.395952	419.909233	7.199347
6.026720	425.856748	7.204352
6.060003	419.292969	7.209357
5.680730	414.712581	7.214362
6.200391	420.153496	7.219366
6.100846	402.666380	7.224371
5.380481	401.317509	7.229376
5.558807	402.198912	7.234381
6.141251	413.565086	7.239386
5.954078	425.238995	7.244390
6.108305	416.106943	7.249395
5.808446	416.078148	7.254400
5.703121	414.385631	7.259405
5.853302	413.141998	7.264410
5.831659	432.718926	7.269414
5.937713	422.546610	7.274419
5.914182	421.958743	7.279424
5.762120	419.446816	7.284429
5.730304	421.500552	7.289434
5.662695	431.096346	7.294438
6.107188	417.394914	7.299443
5.927515	427.618230	7.304448
6.060383	418.709512	7.309453
5.754653	422.301083	7.314458
5.522386	422.671724	7.319462
5.973252	422.339902	7.324467
6.042684	428.800350	7.329472
6.028585	422.235915	7.334477
6.219309	434.555830	7.339482
5.637580	427.972534	7.344486
6.260851	423.689654	7.349491
6.031592	429.894912	7.354496
5.929465	423.355581	7.359501
5.726980	402.426595	7.364506
5.734905	419.895275	7.369510
5.903548	415.942160	7.374515
5.968630	421.798464	7.379520
6.128984	421.771355	7.384525
5.968494	424.195401	7.389530
5.748135	398.847904	7.394534
5.967998	407.948278	7.399539
5.951400	401.973834	7.404544
5.640593	408.460510	7.409549
6.026712	408.215551	7.414554
5.814402	424.398149	7.419558
6.223732	410.730946	7.424563
5.869911	399.884464	7.429568
6.212471	402.481286	7.434573
5.791974	393.845558	7.439578
5.564906	387.777945	7.444582
5.757234	395.426406	7.449587
5.882742	401.347004	7.454592
5.830022	412.528292	7.459597
5.912310	409.102856	7.464602
5.734007	426.684303	7.469606
5.984493	416.247796	7.474611
6.026513	428.906401	7.479616
5.811970	424.967281	7.484621
5.959739	415.706761	7.489626
5.947121	419.370350	7.494630
6.006337	411.410844	7.499635
5.420030	406.649307	7.504640
6.058489	411.330370	7.509645
6.010344	419.096818	7.514650
5.817199	421.430169	7.519654
5.684487	410.867277	7.524659
5.811337	433.780975	7.529664
5.731796	427.558246	7.534669
5.808449	423.717705	7.539674
5.720894	425.321310	7.544678
5.866430	420.563131	7.549683
6.063442	424.952223	7.554688
6.250056	428.308526	7.559693
6.169832	424.879557	7.564698
6.173762	425.695270	7.569702
6.213138	410.541095	7.574707
6.219061	397.944198	7.579712
5.834544	405.467004	7.584717
5.660502	397.883456	7.589722
5.614568	403.260578	7.594726
5.772612	393.940561	7.599731
5.787274	394.325148	7.604736
5.590882	402.218787	7.609741
5.704733	407.894575	7.614746
5.711401	416.553876	7.619750
5.958640	424.469021	7.624755
5.979790	429.894062	7.629760
5.988777	425.766958	7.634765
5.980971	432.052824	7.639770
6.100847	434.036111	7.644774
6.296499	428.494210	7.649779
5.834216	408.980850	7.654784
5.819933	404.134647	7.659789
5.692571	403.692883	7.664794
5.540081	409.665246	7.669798
6.034356	427.505307	7.674803
5.609385	427.566839	7.679808
5.511869	431.790819	7.684813
6.147313	426.011384	7.689818
6.115114	432.162176	7.694822
6.220537	423.425312	7.699827
6.107059	424.969765	7.704832
6.090687	405.702167	7.709837
5.988901	400.404572	7.714842
5.997443	405.266192	7.719846
5.713848	399.462546	7.724851
6.059169	383.645480	7.729856
5.777972	398.352493	7.734861
6.197825	394.323241	7.739866
5.824909	390.025051	7.744870
5.921193	390.657192	7.749875
5.850678	397.460301	7.754880
5.935557	395.227387	7.759885
5.911809	398.486940	7.764890
5.807748	403.673100	7.769894
6.248514	390.502781	7.774899
6.039972	384.507283	7.779904
6.092282	397.242988	7.784909
5.820415	388.060811	7.789914
5.955898	386.542584	7.794918
5.992013	392.478149	7.799923
6.001892	389.237726	7.804928
5.846133	391.368372	7.809933
5.842245	384.522477	7.814938
5.825637	392.473514	7.819942
5.988104	387.325323	7.824947
5.629434	395.180170	7.829952
5.770479	395.626940	7.834957
6.040916	383.262973	7.839962
5.761057	395.784043	7.844966
5.755069	392.919457	7.849971
5.452391	393.486319	7.854976
5.679982	398.072397	7.859981
5.933484	393.619876	7.864986
5.380712	410.319940	7.869990
6.066175	405.501740	7.874995
6.091860	423.242344	7.880000
5.811496	415.101193	7.885005
5.772181	406.451694	7.890010
5.814342	427.049815	7.895014
6.153790	421.409371	7.900019
5.879063	413.682434	7.905024
5.910709	415.356313	7.910029
5.993280	408.784097	7.915034
5.414143	413.785952	7.920038
6.227646	429.545089	7.925043
6.149495	412.261999	7.930048
6.116632	408.864373	7.935053
5.823551	405.122526	7.940058
5.641612	402.629549	7.945062
5.761127	405.319466	7.950067
5.756786	409.233158	7.955072
5.875525	417.255267	7.960077
5.976090	424.352622	7.965082
5.833813	423.005292	7.970086
6.039362	418.936963	7.975091
5.824042	420.972979	7.980096
5.771265	426.003082	7.985101
5.916432	416.847271	7.990106
6.024365	434.047472	7.995110
5.858972	428.390517	8.000115
5.812427	419.201925	8.005133
5.882687	428.596383	8.010150
6.043407	420.226883	8.015168
5.800987	422.850930	8.020186
6.411268	424.217565	8.025203
5.928363	412.595399	8.030221
5.802212	396.307293	8.035238
5.625900	398.127274	8.040256
5.960849	415.557366	8.045274
6.051566	411.819722	8.050291
5.949809	404.981972	8.055309
5.855940	403.893373	8.060326
6.109384	409.892514	8.065344
6.157113	404.943336	8.070362
6.313438	390.472233	8.075379
5.891967	392.623709	8.080397
5.720790	406.440191	8.085414
6.060268	393.564949	8.090432
5.966745	405.827783	8.095450
5.793808	393.284612	8.100467
6.141717	403.358409	8.105485
6.172554	392.743154	8.110502
6.083639	397.068725	8.115520
6.091804	401.347748	8.120538
5.910995	388.609761	8.125555
5.831591	395.110854	8.130573
5.524063	405.000316	8.135590
6.212691	409.025383	8.140608
5.758803	419.466095	8.145626
5.729047	421.234600	8.150643
6.002758	417.259178	8.155661
5.949579	420.706593	8.160678
6.474568	426.585094	8.165696
6.307275	429.572534	8.170714
6.292725	420.104185	8.175731
6.282213	419.827324	8.180749
5.531574	407.974367	8.185766
6.057956	408.711104	8.190784
6.036052	424.260434	8.195802
6.025944	428.475963	8.200819
6.170606	427.530778	8.205837
6.107652	427.287971	8.210854
6.633715	426.915449	8.215872
6.100946	426.889919	8.220890
6.052866	405.866375	8.225907
6.012849	420.630870	8.230925
5.835711	425.457146	8.235942
6.406581	422.901890	8.240960
5.860547	431.492780	8.245978
6.072487	438.337590	8.250995
6.216353	435.727630	8.256013
5.900538	429.782446	8.261030
6.322872	431.873893	8.266048
6.185444	427.090909	8.271066
6.229883	418.672530	8.276083
6.457610	426.318001	8.281101
6.139483	426.745676	8.286118
6.244396	414.418720	8.291136
6.337798	430.057245	8.296154
6.420300	433.822720	8.301171
6.503566	419.524162	8.306189
6.124174	404.489256	8.311206
6.081150	395.101990	8.316224
6.101098	398.114571	8.321242
6.057851	401.025612	8.326259
6.395866	413.812385	8.331277
6.245649	420.431369	8.336294
6.340520	406.253025	8.341312
6.286998	406.072623	8.346330
6.200152	398.650941	8.351347
6.054789	403.656664	8.356365
5.988238	411.416002	8.361382
6.188478	407.280615	8.366400
6.266651	421.113469	8.371418
6.018079	418.864170	8.376435
6.324347	421.380714	8.381453
6.272376	426.983775	8.386470
6.667687	412.128545	8.391488
6.347740	428.231948	8.396506
6.205709	428.827823	8.401523
6.555072	421.389149	8.406541
6.409773	424.863007	8.411558
6.332533	416.122783	8.416576
6.443597	421.746625	8.421594
6.311022	419.657941	8.426611
6.412230	413.101933	8.431629
6.364275	416.928030	8.436646
6.266959	416.597418	8.441664
6.261604	418.714375	8.446682
6.289925	423.873056	8.451699
6.339593	419.971560	8.456717
6.231215	428.586951	8.461734
6.207195	426.767667	8.466752
6.283791	431.986863	8.471770
6.135920	423.248663	8.476787
6.470538	423.637743	8.481805
6.024651	419.721706	8.486822
6.361976	420.953565	8.491840
6.363713	428.912803	8.496858
6.082279	423.505034	8.501875
6.560432	426.028698	8.506893
6.078239	433.422772	8.511910
6.562496	423.826722	8.516928
6.093612	427.322174	8.521946
6.231299	432.638731	8.526963
6.332092	425.916090	8.531981
6.190717	430.301510	8.536998
6.681471	434.943807	8.542016
6.414561	436.715982	8.547034
6.577661	440.848473	8.552051
7.039128	436.280915	8.557069
6.464631	432.973308	8.562087
6.255757	431.180341	8.567104
6.696093	424.337526	8.572122
6.385535	431.956627	8.577139
6.385738	427.725875	8.582157
6.315614	425.109754	8.587175
6.667592	422.004379	8.592192
6.611274	427.655885	8.597210
6.115876	438.629441	8.602227
6.527276	435.757893	8.607245
6.385348	445.128089	8.612263
6.736961	458.522760	8.617280
6.776708	451.472964	8.622298
6.766793	442.317254	8.627315
6.811339	429.272658	8.632333
6.629870	425.347954	8.637351
6.819096	418.444300	8.642368
6.876631	416.499063	8.647386
6.605298	411.735457	8.652403
6.758004	419.494679	8.657421
6.486251	435.782703	8.662439
6.630530	415.322507	8.667456
6.715689	431.489646	8.672474
6.594221	429.315875	8.677491
6.691229	414.292565	8.682509
6.367189	425.115870	8.687527
6.711183	424.377063	8.692544
6.505523	426.007745	8.697562
6.363945	437.400090	8.702579
6.859409	417.363741	8.707597
6.653490	433.899391	8.712615
6.695981	418.384897	8.717632
6.855613	426.178010	8.722650
6.512753	432.023691	8.727667
6.556959	420.129999	8.732685
6.132185	433.665156	8.737703
6.554488	424.959277	8.742720
6.764902	429.331433	8.747738
6.365308	436.610797	8.752755
6.917614	439.698367	8.757773
6.872777	443.105736	8.762791
6.838394	438.646887	8.767808
6.461075	424.776531	8.772826
6.200865	435.216342	8.777843
6.850423	452.191813	8.782861
6.591958	452.651058	8.787879
6.737016	452.859993	8.792896
6.854412	457.661911	8.797914
6.655210	454.133257	8.802931
7.111246	453.328501	8.807949
6.921737	456.004231	8.812967
6.856082	454.749385	8.817984
6.715964	449.255963	8.823002
6.577791	452.140190	8.828019
7.079905	450.576796	8.833037
6.699385	455.110088	8.838055
6.828841	456.632352	8.843072
6.882407	451.608981	8.848090
6.752747	463.442885	8.853107
6.605815	445.787581	8.858125
6.452839	457.701794	8.863143
6.509321	463.891347	8.868160
6.394187	460.095504	8.873178
6.752899	463.532624	8.878195
6.807660	456.221933	8.883213
6.778667	458.110173	8.888231
6.784695	458.610139	8.893248
6.700624	454.637449	8.898266
6.416262	465.946544	8.903283
6.935667	461.468890	8.908301
6.885608	463.379211	8.913319
6.782981	471.891925	8.918336
6.978041	466.036870	8.923354
6.844305	486.278869	8.928371
7.169819	477.658430	8.933389
6.965028	472.229417	8.938407
6.691725	469.014714	8.943424
6.924546	469.421109	8.948442
7.116318	478.276629	8.953459
7.259425	467.886516	8.958477
7.071327	462.203422	8.963495
6.921655	470.548159	8.968512
6.999481	457.794631	8.973530
6.866517	466.182658	8.978547
7.030583	453.859769	8.983565
6.863099	458.888749	8.988583
6.690263	461.183850	8.993600
7.143386	467.662112	8.998618
6.949780	464.743722	9.003635
7.130325	456.001121	9.008653
6.493485	465.975057	9.013671
6.935353	488.231141	9.018688
7.082407	485.415472	9.023706
6.942291	495.388818	9.028723
7.243476	484.397787	9.033741
6.837189	479.807317	9.038759
7.166891	493.388180	9.043776
7.375564	486.842920	9.048794
7.026236	483.987654	9.053811
7.069441	472.655290	9.058829
6.934626	476.031483	9.063847
7.155039	489.177545	9.068864
7.011579	493.053393	9.073882
7.305944	488.088031	9.078899
7.084835	482.026016	9.083917
6.949527	476.261176	9.088935
7.122265	482.537112	9.093952
7.278116	484.096445	9.098970
7.361257	481.791038	9.103987
7.034708	476.956730	9.109005
6.972849	478.723955	9.114023
7.147423	479.983994	9.119040
7.090595	481.145985	9.124058
6.762748	482.744219	9.129075
6.966180	488.924257	9.134093
7.249138	495.341301	9.139111
7.028060	500.076458	9.144128
7.209659	492.766831	9.149146
6.963028	492.839063	9.154163
7.050334	492.835148	9.159181
7.300739	480.632882	9.164199
7.087648	493.521228	9.169216
7.246153	487.711568	9.174234
6.906786	497.195313	9.179251
7.175858	491.637796	9.184269
7.443770	484.809082	9.189287
7.134213	491.707527	9.194304
7.127734	487.553142	9.199322
6.877339	492.052640	9.204339
6.777958	499.315484	9.209357
7.149180	491.614064	9.214375
6.910404	502.112373	9.219392
7.473836	513.702177	9.224410
7.508240	530.856249	9.229427
7.302128	513.872028	9.234445
7.553241	503.789172	9.239463
7.311588	504.770236	9.244480
7.640400	487.007234	9.249498
7.261995	495.990153	9.254515
7.399059	493.001760	9.259533
7.356745	487.322216	9.264551
7.298114	495.681345	9.269568
7.420715	486.856195	9.274586
7.346728	493.919507	9.279603
7.195834	498.692956	9.284621
7.410776	491.420527	9.289639
7.031301	493.094603	9.294656
7.419738	495.831685	9.299674
7.420089	491.057795	9.304691
7.523705	492.657349	9.309709
7.477000	488.527816	9.314727
7.438563	485.587518	9.319744
7.442507	489.084158	9.324762
7.127608	489.724348	9.329779
6.962940	490.167601	9.334797
7.396220	509.966983	9.339815
7.289290	521.012690	9.344832
7.535377	518.864269	9.349850
7.554036	534.993107	9.354867
7.456245	521.985634	9.359885
7.381253	523.873120	9.364903
7.274933	527.296966	9.369920
7.303107	516.888617	9.374938
7.268311	531.556410	9.379955
7.305592	527.764589	9.384973
7.688226	532.596304	9.389991
7.374923	534.804318	9.395008
7.774214	521.735264	9.400026
7.619135	535.081383	9.405043
7.489833	528.191252	9.410061
7.628962	533.078954	9.415079
7.171800	540.659357	9.420096
7.695469	520.155217	9.425114
7.408198	540.177041	9.430131
7.259286	535.087814	9.435149
7.400447	522.064665	9.440167
7.283441	534.183679	9.445184
7.153711	520.285605	9.450202
7.210610	532.382962	9.455219
7.334731	522.530290	9.460237
7.335352	533.933452	9.465255
7.751439	551.874495	9.470272
7.986880	557.085294	9.475290
7.962979	545.038326	9.480307
7.923781	527.779507	9.485325
7.833897	532.295296	9.490343
7.766040	537.407620	9.495360
7.623362	525.106435	9.500378
7.752662	533.403234	9.505395
7.546950	525.382265	9.510413
7.722216	528.944578	9.515431
7.158412	534.471863	9.520448
7.552064	532.338612	9.525466
7.352336	529.445330	9.530483
7.200870	534.446102	9.535501
7.555730	539.256135	9.540519
7.664441	557.217967	9.545536
7.842063	550.193263	9.550554
7.691399	553.820073	9.555571
7.585640	561.176994	9.560589
7.964471	557.578179	9.565607
7.808972	565.659318	9.570624
7.870911	558.318560	9.575642
7.919398	559.557326	9.580659
7.644741	550.577166	9.585677
7.769477	547.767438	9.590695
7.443388	559.459601	9.595712
7.614265	557.870048	9.600730
8.010614	564.569896	9.605747
7.660642	558.700667	9.610765
7.417830	553.622917	9.615783
7.148253	567.090720	9.620800
7.360629	566.735888	9.625818
7.350905	564.310017	9.630835
7.664473	561.508638	9.635853
8.187356	567.875041	9.640871
7.719400	573.307874	9.645888
7.773469	567.684307	9.650906
7.735466	561.532957	9.655923
7.811151	585.038925	9.660941
8.218240	581.208708	9.665959
8.177723	565.948679	9.670976
8.062529	571.013336	9.675994
8.014163	564.457578	9.681011
7.895938	572.201526	9.686029
7.858656	565.914846	9.691047
7.427521	563.565407	9.696064
8.025983	556.690990	9.701082
8.032212	567.731610	9.706099
7.948809	566.734460	9.711117
7.743357	565.655039	9.716135
7.762838	564.749230	9.721152
7.829171	571.006180	9.726170
8.062266	555.528243	9.731187
7.759153	560.476442	9.736205
8.112490	579.078247	9.741223
7.701894	582.450344	9.746240
7.939869	598.971758	9.751258
8.235063	587.490306	9.756275
8.191740	588.922164	9.761293
7.983090	570.838125	9.766311
7.534524	571.294150	9.771328
7.960405	570.089435	9.776346
8.049858	582.622603	9.781363
8.046608	595.584799	9.786381
8.226683	583.090494	9.791399
7.792905	595.109966	9.796416
8.057267	596.213474	9.801434
8.256782	592.063003	9.806451
8.010458	603.628655	9.811469
8.309895	585.239418	9.816487
7.974013	593.904897	9.821504
8.110237	596.018556	9.826522
7.923358	593.431443	9.831539
7.861015	596.090905	9.836557
8.104463	586.935848	9.841575
8.111715	590.047888	9.846592
8.281615	585.154628	9.851610
8.318173	597.610051	9.856627
8.181847	599.445883	9.861645
8.224990	584.221804	9.866663
8.144808	591.261780	9.871680
8.310242	593.772696	9.876698
8.432135	591.604639	9.881715
7.939649	599.435348	9.886733
8.275562	594.837124	9.891751
8.324365	598.467588	9.896768
7.797605	591.403692	9.901786
8.253086	594.474132	9.906803
8.250765	594.226420	9.911821
8.553639	592.640143	9.916839
8.108711	586.146270	9.921856
8.347659	595.772645	9.926874
8.342096	591.825224	9.931891
8.043748	604.066664	9.936909
8.291398	590.779845	9.941927
8.330325	597.092998	9.946944
8.072618	606.448968	9.951962
8.157809	589.235653	9.956979
7.926198	597.169478	9.961997
8.012269	590.583817	9.967015
8.339392	591.488702	9.972032
8.090126	591.723936	9.977050
8.306974	586.190858	9.982067
7.971814	596.314096	9.987085
7.758635	588.761459	9.992103
8.288115	591.034099	9.997120
7.997654	598.182928	10.002138
8.413335	609.883622	10.007155
8.544409	624.744521	10.012173
8.821437	612.717538	10.017191
8.458940	607.323691	10.022208
8.319901	595.408977	10.027226
8.557978	595.190420	10.032243
8.403481	594.415801	10.037261
8.498572	589.156041	10.042279
8.553776	604.140460	10.047296
8.294957	601.943211	10.052314
8.621127	599.509059	10.057331
8.163927	599.966216	10.062349
8.371236	595.170786	10.067367
8.591150	590.256073	10.072384
8.325674	589.851692	10.077402
8.530222	587.645178	10.082419
8.021092	603.628779	10.087437
8.502233	596.368991	10.092455
8.513092	594.014600	10.097472
8.413837	589.922459	10.102490
8.642313	600.103507	10.107507
8.195422	609.185096	10.112525
8.245907	618.719131	10.117543
8.366582	627.326301	10.122560
8.189749	626.744016	10.127578
8.429349	622.303602	10.132595
8.275369	626.646583	10.137613
8.408834	625.764544	10.142631
8.707398	631.027128	10.147648
8.582388	623.692829	10.152666
8.914848	620.181076	10.157683
8.416267	618.106010	10.162701
8.807654	608.404647	10.167719
8.673099	619.518757	10.172736
8.577940	620.225373	10.177754
9.180559	623.485635	10.182771
8.550606	618.386917	10.187789
8.823209	627.738710	10.192807
8.509047	628.693583	10.197824
8.708007	633.199061	10.202842
8.846335	616.654064	10.207859
8.844377	622.395654	10.212877
8.968971	624.747905	10.217895
8.678617	613.391442	10.222912
8.406196	617.609732	10.227930
8.799059	625.925315	10.232947
8.939000	630.222578	10.237965
8.690859	622.212112	10.242983
8.646730	614.976338	10.248000
8.758626	623.329398	10.253018
8.959404	615.671041	10.258035
8.480479	614.435669	10.263053
8.548688	628.374961	10.268071
8.848812	624.736688	10.273088
8.822444	613.874780	10.278106
8.863283	620.800694	10.283123
8.713482	631.890369	10.288141
8.779094	622.651711	10.293159
8.571752	634.482937	10.298176
8.668055	622.442515	10.303194
8.841207	619.161970	10.308211
8.973389	629.474283	10.313229
9.007972	613.980088	10.318247
9.274769	623.518036	10.323264
9.152336	617.541608	10.328282
9.050903	600.958707	10.333299
8.610811	601.012330	10.338317
8.429385	597.020363	10.343335
8.841434	614.863151	10.348352
9.052458	629.479885	10.353370
9.312379	622.800039	10.358387
9.142586	609.953770	10.363405
8.857491	600.359976	10.368423
9.060957	585.279544	10.373440
8.785404	590.572242	10.378458
9.007660	587.692267	10.383475
8.873619	597.230509	10.388493
8.774071	597.888057	10.393511
9.089313	584.739551	10.398528
8.650927	599.751708	10.403546
8.955335	600.945626	10.408563
9.129511	613.976724	10.413581
9.011602	622.357330	10.418599
9.096648	616.528271	10.423616
8.821145	612.496249	10.428634
8.839566	618.619530	10.433651
8.953354	623.946402	10.438669
8.950273	629.475820	10.443687
9.063880	619.448088	10.448704
9.139889	627.470532	10.453722
9.279125	631.081925	10.458739
9.302067	627.804651	10.463757
9.036801	618.467753	10.468775
9.343376	614.304996	10.473792
9.009784	614.395536	10.478810
8.766304	599.322233	10.483827
8.797635	605.662131	10.488845
8.973423	619.122213	10.493863
9.128751	616.531978	10.498880
8.913177	630.947612	10.503898
9.083675	625.628341	10.508915
8.977357	618.201603	10.513933
8.965547	625.632873	10.518951
8.862120	618.610991	10.523968
9.084751	622.816944	10.528986
9.188821	628.832983	10.534003
8.759045	635.425341	10.539021
8.838489	622.932184	10.544039
9.191666	629.499263	10.549056
8.946222	650.735533	10.554074
9.172758	651.735967	10.559091
9.145448	660.005871	10.564109
9.141289	660.470822	10.569127
9.432253	650.455089	10.574144
9.170105	654.894777	10.579162
9.061529	653.920478	10.584179
9.219664	659.039974	10.589197
9.081560	655.435342	10.594215
9.309671	647.034409	10.599232
9.340551	664.423714	10.604250
9.375774	653.065573	10.609267
9.577316	659.880022	10.614285
9.331450	661.818003	10.619303
9.664750	658.311613	10.624320
9.384706	666.103114	10.629338
9.301783	654.009428	10.634355
9.582427	659.951033	10.639373
9.248369	657.875932	10.644391
9.272911	658.234584	10.649408
9.568551	662.187585	10.654426
9.196143	661.280995	10.659443
8.964666	659.122616	10.664461
9.084981	668.116506	10.669479
9.162432	653.539710	10.674496
9.260606	653.657794	10.679514
8.994550	660.031608	10.684531
9.024803	661.943442	10.689549
9.065589	673.415743	10.694567
9.515492	666.121821	10.699584
9.407593	676.401218	10.704602
9.414543	671.038500	10.709619
9.823791	671.917518	10.714637
9.419769	676.485755	10.719655
9.531980	687.392729	10.724672
9.462657	683.081584	10.729690
9.549061	678.545727	10.734707
9.732672	678.079626	10.739725
9.794104	679.321478	10.744743
10.009586	669.483037	10.749760
9.486992	668.858106	10.754778
9.545587	653.506035	10.759795
9.797582	653.255164	10.764813
9.559852	663.918732	10.769831
9.856689	645.165456	10.774848
9.351864	653.823659	10.779866
9.451219	655.661486	10.784883
9.498798	653.491629	10.789901
9.543696	656.021393	10.794919
9.564249	652.376372	10.799936
9.617364	663.508309	10.804954
9.626059	670.175829	10.809971
10.008599	672.764735	10.814989
9.461232	669.803705	10.820007
9.655704	647.778024	10.825024
9.391045	655.223737	10.830042
9.700533	674.240403	10.835059
9.577830	679.517614	10.840077
9.490387	678.899101	10.845095
9.774351	682.042974	10.850112
9.881482	683.582629	10.855130
9.854627	670.747621	10.860147
9.925256	681.978823	10.865165
9.672420	689.691837	10.870183
9.877544	683.423896	10.875200
10.014905	688.123492	10.880218
9.828704	674.937624	10.885235
9.648683	668.656482	10.890253
9.638216	676.764588	10.895271
9.964749	672.028550	10.900288
9.745764	687.941556	10.905306
9.839214	683.893120	10.910323
9.900340	678.264016	10.915341
9.963750	684.483609	10.920359
9.968205	675.245087	10.925376
9.962044	685.121924	10.930394
9.756670	678.659277	10.935411
9.996081	685.671869	10.940429
9.974316	685.699559	10.945447
10.057503	680.296095	10.950464
9.957229	665.624470	10.955482
9.629986	654.976692	10.960499
10.018157	667.853302	10.965517
9.847507	679.111779	10.970535
10.142911	674.493362	10.975552
10.103325	672.495358	10.980570
9.800757	668.320184	10.985587
10.384274	664.962169	10.990605
10.054157	658.986392	10.995623
9.363602	652.564770	11.000640
10.066570	673.639320	11.005658
10.059471	673.773128	11.010675
10.454835	685.164011	11.015693
9.836638	665.119000	11.020711
9.435485	664.861621	11.025728
10.167651	679.177458	11.030746
10.037435	684.992914	11.035763
10.103589	684.663032	11.040781
9.647557	678.721734	11.045799
9.677019	677.366816	11.050816
9.900126	683.246201	11.055834
10.014571	675.935777	11.060851
10.031751	678.199114	11.065869
9.772767	685.179231	11.070887
10.041990	680.037387	11.075904
9.911127	689.544754	11.080922
9.969814	682.666195	11.085939
10.344129	693.891009	11.090957
10.159364	699.900982	11.095975
10.120613	690.097457	11.100992
10.000727	695.413669	11.106010
10.062504	710.167621	11.111027
10.639096	707.894490	11.116045
10.351604	707.669695	11.121063
9.919290	683.812287	11.126080
10.558986	693.101486	11.131098
10.082339	687.291618	11.136115
10.235085	691.327481	11.141133
10.094864	701.935599	11.146151
10.509248	697.267007	11.151168
10.112016	690.747691	11.156186
10.122827	704.255875	11.161203
10.528701	705.304416	11.166221
10.446075	718.916620	11.171239
10.179389	707.902075	11.176256
10.403476	703.366189	11.181274
10.098032	716.146876	11.186291
10.477519	708.530974	11.191309
10.208053	723.737439	11.196327
10.103571	705.872300	11.201344
10.050526	710.709648	11.206362
9.973733	719.312108	11.211379
10.238763	720.524352	11.216397
10.236288	714.769256	11.221415
10.143636	715.981172	11.226432
10.385166	716.754372	11.231450
10.065683	716.836479	11.236467
10.281644	719.348218	11.241485
10.141156	733.072535	11.246503
10.512228	746.819392	11.251520
10.577282	747.040175	11.256538
10.684723	745.238885	11.261555
10.803234	742.295037	11.266573
10.452768	729.510410	11.271591
10.383194	722.869425	11.276608
10.558692	721.778307	11.281626
10.354559	747.403400	11.286643
10.495786	730.455220	11.291661
11.040192	741.066049	11.296679
10.670831	733.304549	11.301696
10.582863	712.109751	11.306714
10.391290	721.735418	11.311731
10.437924	722.592391	11.316749
10.291627	734.750156	11.321767
10.570233	750.161588	11.326784
10.789816	744.476259	11.331802
10.596528	752.712040	11.336819
10.973619	740.276371	11.341837
10.467760	743.318838	11.346855
10.824059	750.742868	11.351872
10.638295	744.230307	11.356890
10.680869	756.181909	11.361907
10.795461	747.374073	11.366925
10.809078	743.711578	11.371943
10.516628	737.920552	11.376960
10.759238	735.783107	11.381978
10.639639	750.710352	11.386995
10.816455	742.039944	11.392013
10.845168	754.899274	11.397031
10.817419	744.376415	11.402048
11.092780	742.376639	11.407066
10.560233	744.547601	11.412083
10.747892	724.712578	11.417101
10.939412	728.054282	11.422119
10.540985	721.431627	11.427136
10.887446	726.376546	11.432154
10.757427	737.953388	11.437171
11.091869	729.212163	11.442189
10.826987	736.195737	11.447207
10.526037	731.321101	11.452224
10.924685	734.547489	11.457242
10.558951	744.577274	11.462259
10.835675	746.412567	11.467277
11.358258	742.401641	11.472295
11.007192	750.621476	11.477312
11.094097	740.222951	11.482330
10.749563	733.281995	11.487347
11.114312	736.675373	11.492365
10.887133	727.362128	11.497383
10.870744	728.653157	11.502400
11.303785	735.272719	11.507418
10.708969	721.263170	11.512435
11.128248	740.440284	11.517453
11.048415	730.522482	11.522471
10.732334	724.171301	11.527488
11.023663	730.992298	11.532506
11.048577	741.792797	11.537523
10.798548	747.164877	11.542541
10.717590	739.111075	11.547559
10.746425	750.190012	11.552576
11.096322	749.610421	11.557594
10.886301	753.216089	11.562611
11.052211	745.920449	11.567629
11.162827	740.743194	11.572647
10.868568	760.818319	11.577664
10.906940	742.774047	11.582682
10.987145	739.019265	11.587699
10.973789	738.265695	11.592717
11.033552	736.136620	11.597735
11.082143	741.685291	11.602752
11.291969	749.348347	11.607770
11.243038	743.805406	11.612787
11.037191	745.393050	11.617805
11.273148	751.103243	11.622823
11.218916	744.978709	11.627840
11.414868	742.882628	11.632858
11.125872	751.155088	11.637875
11.323018	748.684962	11.642893
11.343128	750.654575	11.647911
11.088641	745.396835	11.652928
11.167457	741.671410	11.657946
11.189543	743.679074	11.662963
10.852823	754.244223	11.667981
11.579652	762.939746	11.672999
11.312366	776.274996	11.678016
11.741130	776.617628	11.683034
11.554118	763.860083	11.688051
11.196764	754.971309	11.693069
11.482054	750.209490	11.698087
11.430725	745.906375	11.703104
11.809413	734.242642	11.708122
11.379090	742.930405	11.713139
11.498085	747.865884	11.718157
11.548670	736.676271	11.723175
11.486096	744.786431	11.728192
11.397663	751.089007	11.733210
11.046432	744.565413	11.738227
11.434692	751.252214	11.743245
11.534465	740.974177	11.748263
11.252185	740.665661	11.753280
11.424365	744.283446	11.758298
11.337423	749.443768	11.763315
11.451655	756.491349	11.768333
11.735094	760.914708	11.773351
11.380676	755.870194	11.778368
11.599439	740.743291	11.783386
11.620787	748.493390	11.788403
11.571111	751.097154	11.793421
11.573807	743.885169	11.798439
11.302338	753.512447	11.803456
11.491700	758.050646	11.808474
11.716793	779.425631	11.813491
11.226019	776.515845	11.818509
11.759779	774.710227	11.823527
11.782335	780.311335	11.828544
11.562176	774.714215	11.833562
11.489664	774.437555	11.838579
11.727114	773.102086	11.843597
11.840616	777.908094	11.848615
11.714447	788.115598	11.853632
11.908219	772.577124	11.858650
12.048997	774.014985	11.863667
11.538501	755.211269	11.868685
11.692839	761.461527	11.873703
11.457325	773.070197	11.878720
11.865796	775.929390	11.883738
11.871654	777.802659	11.888755
11.653975	768.926812	11.893773
11.581651	775.541736	11.898791
11.569996	783.057587	11.903808
11.530481	783.981548	11.908826
11.514684	777.676961	11.913843
11.718478	780.924736	11.918861
11.768009	780.422829	11.923879
11.608261	786.483611	11.928896
12.010334	778.304401	11.933914
11.770510	775.867417	11.938931
11.712417	775.914003	11.943949
12.256251	762.036459	11.948967
11.871831	777.089074	11.953984
12.037814	766.493246	11.959002
12.063036	775.710158	11.964019
11.989438	777.557589	11.969037
12.085319	767.913621	11.974055
11.723672	786.101947	11.979072
11.789548	769.606548	11.984090
11.750104	781.586583	11.989107
11.605722	781.112687	11.994125
12.123527	778.922475	11.999143
11.688251	780.120165	12.004160
11.986864	784.520162	12.009178
12.292233	801.330600	12.014195
11.957489	797.097334	12.019213
12.225249	805.181965	12.024231
11.804468	801.164553	12.029248
12.267038	802.918066	12.034266
12.253598	808.831277	12.039283
11.822442	797.088771	12.044301
12.126243	792.032104	12.049319
11.984470	806.264774	12.054336
12.081950	798.186373	12.059354
12.337493	798.784066	12.064371
12.254311	794.577719	12.069389
12.238350	792.668198	12.074407
12.151373	800.112860	12.079424
12.253962	789.237193	12.084442
12.051533	802.390225	12.089459
12.084041	798.813751	12.094477
12.608539	793.660682	12.099495
12.577168	796.439446	12.104512
12.176320	793.797912	12.109530
12.215654	793.435951	12.114547
12.082519	799.524716	12.119565
12.149069	807.846400	12.124583
11.934553	795.454233	12.129600
12.160361	796.448006	12.134618
12.055385	799.584736	12.139635
11.979168	797.903242	12.144653
12.171633	795.828200	12.149671
12.114523	798.690337	12.154688
12.343892	804.974661	12.159706
12.236947	800.409119	12.164723
11.990131	803.143286	12.169741
12.499031	811.736000	12.174759
12.736606	816.113323	12.179776
12.431688	808.474379	12.184794
12.550740	800.725814	12.189811
12.380673	809.820127	12.194829
12.521910	796.847315	12.199847
12.438950	807.775017	12.204864
12.412040	801.401995	12.209882
12.636076	796.150181	12.214899
12.700326	807.477983	12.219917
12.725002	794.397491	12.224935
12.413143	799.507024	12.229952
12.288645	797.613570	12.234970
12.325642	798.240983	12.239987
12.317553	813.112860	12.245005
12.424077	817.007801	12.250023
12.570782	832.911794	12.255040
12.518470	839.188460	12.260058
12.927289	828.286563	12.265075
12.646710	837.518229	12.270093
13.044053	829.970563	12.275111
12.442870	817.305725	12.280128
12.534006	821.072919	12.285146
12.771674	823.236663	12.290163
12.876223	837.142881	12.295181
12.894722	816.833917	12.300199
12.759691	808.410542	12.305216
12.415442	799.118962	12.310234
12.907477	810.139698	12.315251
12.997306	823.063872	12.320269
12.523605	797.948499	12.325287
12.813821	812.838290	12.330304
12.640269	813.339112	12.335322
12.909978	821.183021	12.340339
12.566899	840.901130	12.345357
12.884384	824.522428	12.350375
12.509519	830.518205	12.355392
12.764551	825.193358	12.360410
12.843718	832.581352	12.365427
12.770540	830.600884	12.370445
12.855990	821.292010	12.375463
13.036993	826.058438	12.380480
12.609043	837.366243	12.385498
13.051112	826.484340	12.390515
12.834961	835.546528	12.395533
12.763517	829.344209	12.400551
13.071030	828.714840	12.405568
12.384785	823.878950	12.410586
13.313751	821.373390	12.415603
12.913316	838.518481	12.420621
12.951017	825.160664	12.425639
12.937635	828.752845	12.430656
12.739376	834.150744	12.435674
13.128768	815.682992	12.440691
12.628727	832.549907	12.445709
12.307686	834.985282	12.450727
13.084517	851.183217	12.455744
12.912176	862.926074	12.460762
13.562456	860.979658	12.465779
13.300878	864.067589	12.470797
13.200112	848.065800	12.475815
13.109698	845.885361	12.480832
13.056172	838.371657	12.485850
13.280676	845.809346	12.490867
13.158924	843.901163	12.495885
13.201051	827.664304	12.500903
13.149737	834.024744	12.505920
13.029281	843.708702	12.510938
13.441879	847.656692	12.515955
13.238999	856.547045	12.520973
13.258338	847.884003	12.525991
13.226328	841.742178	12.531008
13.135913	859.658349	12.536026
13.409464	847.806627	12.541043
13.165929	862.952754	12.546061
13.256677	855.186107	12.551079
13.295607	859.582494	12.556096
13.308272	865.975083	12.561114
13.381859	856.936800	12.566131
13.002024	866.634606	12.571149
13.487136	854.653643	12.576167
13.466952	852.762329	12.581184
13.307204	865.361119	12.586202
13.378495	857.250310	12.591219
13.337629	867.237803	12.596237
13.463487	863.690663	12.601255
13.898309	864.112104	12.606272
13.314958	859.832716	12.611290
13.531686	861.190232	12.616307
13.145404	862.950495	12.621325
13.083978	854.169915	12.626343
13.588383	852.191416	12.631360
12.931663	868.489097	12.636378
13.348861	857.492209	12.641395
12.967672	865.094952	12.646413
12.965076	870.527545	12.651431
13.435646	886.958872	12.656448
13.443176	897.304561	12.661466
13.347126	892.976418	12.666483
13.602534	893.463823	12.671501
14.046521	898.339738	12.676519
13.734879	884.458703	12.681536
13.518162	894.536484	12.686554
13.749054	885.915414	12.691571
13.848880	889.116331	12.696589
13.682269	888.986299	12.701607
13.824224	889.917375	12.706624
13.898844	893.350960	12.711642
14.141234	885.013766	12.716659
13.562105	887.095415	12.721677
13.782684	891.230338	12.726695
14.005331	882.982120	12.731712
13.755309	878.766616	12.736730
13.905723	857.792411	12.741747
13.742367	862.299084	12.746765
13.883457	865.498491	12.751783
13.717852	862.090938	12.756800
13.458334	879.601200	12.761818
13.822043	886.173340	12.766835
14.049718	894.550024	12.771853
13.945613	887.912215	12.776871
14.150274	886.021626	12.781888
13.910706	889.571885	12.786906
14.036088	891.213742	12.791923
14.224714	879.487329	12.796941
13.667599	862.408886	12.801959
13.806964	857.218181	12.806976
13.656126	868.914780	12.811994
13.817482	881.760562	12.817011
14.010868	888.021640	12.822029
13.615472	887.480777	12.827047
14.074716	884.872354	12.832064
13.703482	891.742396	12.837082
13.851654	892.984102	12.842099
13.965756	891.300865	12.847117
13.986303	895.959112	12.852135
13.950795	896.712368	12.857152
13.853451	901.840412	12.862170
14.021796	893.569967	12.867187
14.176346	895.674538	12.872205
13.885403	901.786274	12.877223
14.228530	894.727272	12.882240
13.778776	899.352336	12.887258
14.145432	918.048299	12.892275
14.369056	915.017572	12.897293
14.335012	933.968126	12.902311
14.515515	914.613090	12.907328
14.507715	913.417038	12.912346
14.391068	899.146447	12.917363
14.306435	897.616700	12.922381
13.861967	895.827381	12.927399
14.091249	892.997065	12.932416
14.197289	911.822590	12.937434
14.234446	916.194881	12.942451
14.310480	924.182837	12.947469
14.313600	928.132683	12.952487
14.368119	918.479023	12.957504
14.015316	924.057682	12.962522
14.167856	913.737449	12.967539
14.234267	920.357161	12.972557
14.398082	927.404105	12.977575
14.288542	920.388802	12.982592
14.183453	925.768974	12.987610
14.530650	913.659603	12.992627
14.788441	921.225072	12.997645
14.201734	922.663211	13.002663
14.703208	923.696068	13.007680
14.193827	925.681073	13.012698
14.407722	918.092926	13.017715
14.357280	920.261883	13.022733
14.175380	915.385227	13.027751
14.352006	920.246289	13.032768
14.456615	934.700813	13.037786
14.732688	943.592759	13.042803
15.023021	947.148160	13.047821
14.637796	931.831073	13.052839
15.134673	919.894269	13.057856
14.594952	925.421156	13.062874
14.494648	919.882705	13.067891
14.567338	924.325884	13.072909
14.446345	917.278426	13.077927
14.550073	916.001947	13.082944
14.576793	929.649701	13.087962
14.580059	951.081069	13.092979
15.063360	950.303177	13.097997
14.960348	955.884555	13.103015
14.886922	930.196213	13.108032
14.794756	933.539280	13.113050
14.705433	917.901111	13.118067
14.750675	914.968159	13.123085
14.771308	931.777280	13.128103
15.033399	927.881981	13.133120
14.645095	925.843951	13.138138
14.614254	943.928296	13.143155
14.830340	940.040399	13.148173
14.803307	951.397367	13.153191
15.164971	949.587695	13.158208
14.876877	954.091982	13.163226
14.884292	959.189742	13.168243
15.253909	955.379601	13.173261
15.042678	953.791846	13.178279
15.089053	932.556042	13.183296
15.040253	929.044639	13.188314
14.726828	924.241183	13.193331
14.985196	926.465880	13.198349
15.027096	946.619627	13.203367
15.337275	943.391651	13.208384
15.039861	948.778323	13.213402
15.026915	950.754212	13.218419
15.194047	934.753228	13.223437
14.941053	949.393514	13.228455
15.104554	946.869283	13.233472
15.054033	957.449664	13.238490
14.989451	956.160058	13.243507
15.138436	944.210267	13.248525
14.973586	955.445747	13.253543
14.955029	949.973191	13.258560
14.870119	955.718576	13.263578
14.826792	954.283357	13.268595
14.918879	942.415103	13.273613
15.076695	956.798760	13.278631
14.700654	965.047635	13.283648
14.804275	968.718724	13.288666
15.301093	983.188484	13.293683
15.531895	979.493682	13.298701
15.286811	980.552592	13.303719
15.373612	974.302119	13.308736
15.076564	983.440448	13.313754
15.172832	981.027698	13.318771
15.551369	974.708446	13.323789
15.463272	988.791690	13.328807
15.547396	973.199985	13.333824
15.575307	978.185034	13.338842
15.444971	986.089234	13.343859
15.419310	980.854217	13.348877
15.419483	991.820368	13.353895
15.532380	986.541982	13.358912
15.399112	988.202582	13.363930
15.532547	987.851143	13.368947
15.696456	970.993423	13.373965
15.522206	978.128044	13.378983
15.778285	972.499483	13.384000
15.715186	987.304058	13.389018
15.707349	981.856978	13.394035
15.607796	971.192608	13.399053
15.611422	982.509203	13.404071
15.554090	976.454664	13.409088
15.507726	986.001095	13.414106
15.556174	976.135938	13.419123
15.690820	987.188900	13.424141
15.658087	982.938343	13.429159
15.795280	981.199125	13.434176
16.248864	974.734718	13.439194
15.728969	974.300336	13.444211
15.811787	981.740644	13.449229
15.841297	978.081076	13.454247
15.707252	978.048792	13.459264
15.887984	973.820727	13.464282
15.891905	970.974303	13.469299
15.930208	977.916542	13.474317
15.783203	977.265348	13.479335
15.548796	976.980307	13.484352
15.568359	974.038991	13.489370
15.731552	985.059974	13.494387
15.735030	972.038336	13.499405
15.680844	978.762239	13.504423
15.736848	971.803990	13.509440
15.811017	963.479989	13.514458
15.721100	976.015665	13.519475
15.795379	970.235685	13.524493
15.663551	974.978968	13.529511
16.041495	964.137187	13.534528
15.898838	981.937549	13.539546
15.687105	989.723040	13.544563
16.650652	994.180112	13.549581
16.020117	998.058838	13.554599
15.956894	979.238696	13.559616
15.966215	988.943810	13.564634
16.342324	995.396548	13.569651
16.456753	978.388264	13.574669
16.209318	979.021161	13.579687
16.089309	973.670954	13.584704
16.083378	972.672093	13.589722
15.964564	972.689252	13.594739
16.075885	979.049938	13.599757
15.935240	983.913952	13.604775
16.287059	995.588297	13.609792
16.498436	1003.942050	13.614810
16.492838	1010.413787	13.619827
16.411660	995.991502	13.624845
16.086516	998.731956	13.629863
16.041569	1004.376087	13.634880
16.445492	1004.572659	13.639898
15.852597	1011.711039	13.644915
16.108185	1012.408421	13.649933
15.861056	1006.039429	13.654951
15.976113	1007.377546	13.659968
16.216090	1005.731261	13.664986
16.396142	1008.274764	13.670003
16.562446	1008.044938	13.675021
16.256552	1011.603823	13.680039
16.245360	1001.032095	13.685056
16.423673	1020.407228	13.690074
16.157623	1036.644262	13.695091
16.486097	1037.119007	13.700109
16.709370	1030.319572	13.705127
16.763712	1036.087832	13.710144
17.007443	1033.540881	13.715162
16.405737	1019.893945	13.720179
16.693955	1019.479827	13.725197
16.795172	1016.588580	13.730215
16.447034	1014.294829	13.735232
16.828586	1005.484355	13.740250
16.758475	1004.277731	13.745267
16.814787	999.246053	13.750285
16.790518	1005.616856	13.755303
16.410662	1008.476768	13.760320
16.434082	996.501238	13.765338
16.630879	1014.505239	13.770355
16.969243	1019.774765	13.775373
17.097777	1042.162063	13.780391
16.928838	1028.647306	13.785408
17.077247	1000.027802	13.790426
16.773626	1004.766814	13.795443
16.546115	1011.575861	13.800461
16.676216	1012.130624	13.805479
17.042271	999.686630	13.810496
17.042681	1000.245111	13.815514
16.508633	1009.129955	13.820531
16.757011	996.830095	13.825549
17.072020	1033.338538	13.830567
16.953557	1030.430649	13.835584
17.015879	1018.206097	13.840602
16.726563	1023.281373	13.845619
16.904193	1024.871507	13.850637
17.184329	1027.453878	13.855655
17.403451	1030.453349	13.860672
16.871655	1022.047599	13.865690
16.580709	1019.226375	13.870707
17.046526	1019.110213	13.875725
16.930957	1033.188886	13.880743
16.981629	1033.192698	13.885760
16.999338	1033.061038	13.890778
17.176433	1038.173394	13.895795
17.216997	1035.151640	13.900813
17.102328	1041.486028	13.905831
17.020124	1036.272539	13.910848
17.078822	1027.625526	13.915866
16.860894	1042.084249	13.920883
16.901535	1025.070000	13.925901
17.026804	1032.945958	13.930919
16.990051	1025.377726	13.935936
17.187889	1040.847475	13.940954
16.879877	1046.816837	13.945971
17.592548	1045.419738	13.950989
17.400701	1058.320691	13.956007
17.497522	1062.408899	13.961024
17.446333	1062.517129	13.966042
17.250224	1068.956113	13.971059
17.520274	1055.082123	13.976077
17.852052	1056.775997	13.981095
17.723568	1049.909213	13.986112
17.457875	1028.760668	13.991130
17.623026	1033.149728	13.996147
17.706092	1027.934417	14.001165
17.557666	1026.881753	14.006183
17.269067	1032.781673	14.011200
17.965880	1031.969182	14.016218
17.227779	1042.355724	14.021235
17.586249	1030.880215	14.026253
17.632504	1027.049983	14.031271
17.240579	1039.103329	14.036288
17.416863	1030.132407	14.041306
17.065974	1035.353075	14.046323
17.482397	1059.997349	14.051341
17.670294	1065.649176	14.056359
17.422077	1074.163550	14.061376
17.774637	1073.715376	14.066394
17.723493	1071.044540	14.071411
17.740779	1068.842040	14.076429
17.967196	1072.432733	14.081447
17.354342	1073.598777	14.086464
17.862018	1064.929112	14.091482
17.657662	1071.423585	14.096499
17.815943	1061.340060	14.101517
17.955886	1070.908009	14.106535
17.759071	1067.092154	14.111552
17.869701	1062.379769	14.116570
17.888752	1058.938212	14.121587
17.889857	1065.780554	14.126605
17.967983	1067.412427	14.131623
17.687681	1069.831954	14.136640
17.754453	1062.190897	14.141658
17.939300	1074.857004	14.146675
17.820215	1064.278067	14.151693
17.838011	1074.221262	14.156711
17.565097	1069.435471	14.161728
18.038338	1080.243796	14.166746
18.606647	1090.240095	14.171763
18.108635	1083.913417	14.176781
18.309196	1067.826863	14.181799
18.165918	1073.806014	14.186816
18.554176	1057.233019	14.191834
18.054449	1068.178114	14.196851
18.100504	1068.161040	14.201869
18.202234	1066.566330	14.206887
18.022808	1070.216219	14.211904
18.349713	1057.283851	14.216922
18.291985	1066.980315	14.221939
18.227329	1062.133933	14.226957
18.431933	1061.293155	14.231975
18.171833	1065.322061	14.236992
18.570516	1068.840789	14.242010
18.293305	1064.501500	14.247027
17.943782	1064.141797	14.252045
18.346735	1061.350061	14.257063
18.043379	1068.554477	14.262080
18.322783	1077.192647	14.267098
18.235897	1083.379375	14.272115
18.600847	1091.115966	14.277133
18.443173	1090.357100	14.282151
18.383682	1088.689047	14.287168
18.729555	1096.622659	14.292186
18.435464	1086.598918	14.297203
18.531172	1087.110753	14.302221
18.391756	1079.902119	14.307239
18.552284	1094.007846	14.312256
18.747663	1085.135491	14.317274
18.775061	1089.463290	14.322291
17.968811	1087.465965	14.327309
18.619080	1082.694114	14.332327
18.376895	1091.316341	14.337344
18.816762	1095.596841	14.342362
18.701374	1095.363574	14.347379
18.509387	1101.138419	14.352397
18.445914	1082.535675	14.357415
18.639729	1100.754900	14.362432
18.521631	1086.765724	14.367450
18.405010	1090.314703	14.372467
18.460505	1089.552690	14.377485
18.910071	1088.227606	14.382503
18.613573	1094.929016	14.387520
18.787433	1079.584337	14.392538
18.943476	1084.058958	14.397555
18.731923	1088.695491	14.402573
19.223488	1086.579543	14.407591
18.857878	1092.727311	14.412608
18.702547	1098.625800	14.417626
19.007149	1105.771095	14.422643
18.974147	1117.878456	14.427661
19.347195	1097.717779	14.432679
19.154345	1090.922037	14.437696
18.969270	1088.295768	14.442714
18.986092	1090.145220	14.447731
18.732951	1095.112000	14.452749
19.115522	1100.874558	14.457767
19.233387	1111.357840	14.462784
18.975976	1109.077718	14.467802
18.942488	1106.289608	14.472819
19.256082	1118.153699	14.477837
19.582365	1112.068481	14.482855
18.996553	1098.731099	14.487872
19.101624	1103.876636	14.492890
18.866488	1105.646685	14.497907
18.866777	1122.339122	14.502925
19.019651	1122.524241	14.507943
19.261354	1128.794654	14.512960
19.210616	1118.010913	14.517978
19.328458	1120.714593	14.522995
19.177623	1126.340545	14.528013
19.392850	1111.959507	14.533031
19.280038	1117.392982	14.538048
19.420856	1119.575825	14.543066
19.510189	1115.074192	14.548083
19.141781	1127.055326	14.553101
19.546822	1111.054404	14.558119
19.427744	1113.381950	14.563136
19.455626	1113.306866	14.568154
19.426518	1119.035907	14.573171
19.565076	1131.500886	14.578189
19.296042	1114.452296	14.583207
19.302529	1112.821164	14.588224
19.338322	1125.004943	14.593242
19.602724	1120.171081	14.598259
19.386915	1127.266781	14.603277
19.401431	1128.145519	14.608295
19.653017	1136.030177	14.613312
19.714176	1141.839372	14.618330
19.998901	1136.677003	14.623347
19.930755	1141.742732	14.628365
19.799145	1121.905933	14.633383
19.906674	1115.993063	14.638400
19.717867	1113.757303	14.643418
19.971849	1111.314729	14.648435
19.941031	1102.727145	14.653453
20.041517	1111.470873	14.658471
19.787756	1108.922476	14.663488
19.792003	1116.267584	14.668506
19.662201	1112.513465	14.673523
19.490966	1104.866254	14.678541
19.911333	1117.004186	14.683559
20.085813	1131.664046	14.688576
19.854215	1127.594124	14.693594
19.932472	1128.869151	14.698611
19.970462	1140.593009	14.703629
20.222752	1135.292718	14.708647
19.601119	1124.388195	14.713664
20.068283	1137.395233	14.718682
20.103359	1143.007984	14.723699
20.164407	1137.501147	14.728717
20.289680	1140.429943	14.733735
20.064620	1141.286473	14.738752
20.164961	1138.447702	14.743770
20.359158	1132.804314	14.748787
20.142443	1140.316242	14.753805
20.196849	1139.927770	14.758823
20.181830	1139.461612	14.763840
20.415190	1142.585110	14.768858
20.386700	1131.586300	14.773875
20.272951	1135.567814	14.778893
20.261821	1123.307294	14.783911
20.276802	1122.205378	14.788928
20.148028	1133.320872	14.793946
20.435853	1126.811956	14.798963
20.324770	1133.932077	14.803981
20.601090	1122.685493	14.808999
20.499682	1140.346567	14.814016
20.248222	1140.210773	14.819034
20.380998	1122.361247	14.824051
19.937388	1138.230554	14.829069
20.198495	1138.390111	14.834087
20.492074	1131.936532	14.839104
20.504552	1135.265007	14.844122
20.297165	1129.280375	14.849139
20.218517	1137.656740	14.854157
20.246803	1134.417150	14.859175
20.333360	1127.742906	14.864192
20.548199	1150.635305	14.869210
20.665090	1158.290897	14.874227
20.682582	1162.155863	14.879245
20.754158	1172.118379	14.884263
20.560931	1168.124375	14.889280
20.423259	1173.103391	14.894298
20.497268	1163.908781	14.899315
20.617864	1163.237958	14.904333
20.464911	1159.630150	14.909351
20.645835	1172.822294	14.914368
20.459958	1162.477519	14.919386
20.911390	1169.338976	14.924403
20.600370	1178.419994	14.929421
20.319604	1167.980088	14.934439
20.488702	1182.819793	14.939456
20.954419	1202.330209	14.944474
21.216590	1184.291735	14.949491
21.329584	1199.127541	14.954509
21.139464	1181.494667	14.959527
21.118095	1168.319219	14.964544
20.928966	1170.556005	14.969562
21.354118	1156.628343	14.974579
20.715597	1160.300785	14.979597
21.293181	1161.359461	14.984615
21.039454	1163.221945	14.989632
20.869299	1170.045989	14.994650
21.418231	1180.386833	14.999667
21.085818	1190.937692	15.004685
21.665051	1185.832526	15.009703
21.522776	1166.681967	15.014720
21.025375	1163.403674	15.019738
21.463949	1167.579111	15.024755
21.218606	1167.744029	15.029773
21.244167	1155.714192	15.034791
21.358931	1165.635517	15.039808
21.421083	1168.185246	15.044826
21.197244	1159.054818	15.049843
21.454796	1163.487691	15.054861
21.774442	1156.299205	15.059879
21.630381	1154.529195	15.064896
21.169567	1163.125004	15.069914
21.290226	1160.445049	15.074931
21.211531	1166.021304	15.079949
21.555286	1158.511365	15.084967
21.697409	1158.560095	15.089984
21.284808	1152.640464	15.095002
21.594926	1169.618309	15.100019
21.286112	1183.489723	15.105037
21.594640	1195.380101	15.110055
21.647619	1181.364930	15.115072
21.636277	1191.435437	15.120090
21.572632	1187.765824	15.125107
21.756452	1194.179667	15.130125
21.707503	1190.731801	15.135143
21.609218	1188.507247	15.140160
21.765930	1191.334810	15.145178
22.029455	1179.540388	15.150195
21.909081	1186.858691	15.155213
21.678367	1192.132178	15.160231
22.073265	1188.955002	15.165248
21.921391	1193.759235	15.170266
21.610328	1191.100629	15.175283
21.545479	1190.212459	15.180301
21.863288	1185.329403	15.185319
21.976658	1183.965397	15.190336
21.896941	1191.886137	15.195354
21.825142	1179.357887	15.200371
21.872862	1186.549607	15.205389
21.929347	1192.900845	15.210407
22.033255	1185.617901	15.215424
21.760370	1196.568309	15.220442
21.606926	1184.770558	15.225459
21.896068	1193.655963	15.230477
22.079438	1205.856159	15.235495
22.456327	1208.753622	15.240512
21.889504	1196.295355	15.245530
22.207499	1193.206269	15.250547
22.226188	1214.556629	15.255565
21.970966	1220.915105	15.260583
22.376860	1215.753943	15.265600
22.413417	1224.866709	15.270618
22.704420	1210.836974	15.275635
22.444900	1209.510970	15.280653
22.311636	1194.091953	15.285671
22.542034	1186.237800	15.290688
22.311917	1183.427060	15.295706
22.069162	1186.525722	15.300723
21.952742	1200.294502	15.305741
22.165074	1218.056941	15.310759
22.454883	1213.014751	15.315776
22.135125	1219.380546	15.320794
22.161642	1229.030714	15.325811
22.536680	1215.912925	15.330829
22.392694	1221.684213	15.335847
22.540144	1217.651217	15.340864
22.432689	1216.400067	15.345882
22.998540	1213.553830	15.350899
23.065914	1203.247478	15.355917
22.300027	1223.803050	15.360935
22.778579	1210.155248	15.365952
22.607317	1214.188603	15.370970
22.848557	1212.556652	15.375987
22.846088	1209.342598	15.381005
22.444280	1213.862012	15.386023
23.035065	1209.443795	15.391040
22.903465	1206.655938	15.396058
22.992518	1205.610662	15.401075
22.863799	1211.535894	15.406093
22.869768	1211.807092	15.411111
22.936213	1209.448636	15.416128
22.598960	1205.796090	15.421146
23.131974	1210.277140	15.426163
22.965030	1207.129040	15.431181
23.002845	1206.838174	15.436199
23.330564	1207.041637	15.441216
23.093334	1215.484795	15.446234
23.050374	1208.227096	15.451251
22.979772	1211.747832	15.456269
22.829707	1203.600499	15.461287
23.049507	1196.334022	15.466304
23.208203	1208.916387	15.471322
23.163899	1205.607491	15.476339
23.491868	1206.867239	15.481357
22.994261	1214.898578	15.486375
23.216705	1204.741571	15.491392
22.994991	1225.563655	15.496410
23.523365	1215.065776	15.501427
23.483766	1232.381951	15.506445
23.469979	1226.060808	15.511463
23.402075	1212.414545	15.516480
23.402334	1214.477740	15.521498
23.144883	1202.200195	15.526515
23.634488	1213.758349	15.531533
23.254767	1213.519952	15.536551
23.619241	1200.301576	15.541568
23.379202	1215.392951	15.546586
23.365376	1225.240305	15.551603
23.605459	1228.871684	15.556621
23.547606	1225.196578	15.561639
23.715818	1215.068602	15.566656
23.436553	1216.381266	15.571674
23.486013	1225.403528	15.576691
24.159497	1224.087288	15.581709
23.822539	1224.450388	15.586727
23.597902	1210.143524	15.591744
23.913210	1207.140889	15.596762
23.775483	1197.685036	15.601779
23.882564	1200.748129	15.606797
23.532445	1198.562632	15.611815
23.865056	1202.520194	15.616832
23.839747	1211.423723	15.621850
23.835527	1214.850235	15.626867
23.982099	1219.167233	15.631885
23.667019	1219.718420	15.636903
24.016053	1216.178602	15.641920
23.821321	1223.390921	15.646938
23.778497	1225.496074	15.651955
24.192739	1224.440160	15.656973
23.786988	1235.089376	15.661991
23.873024	1220.912038	15.667008
24.191550	1221.648234	15.672026
23.852181	1221.197492	15.677043
24.049444	1223.835121	15.682061
23.996960	1228.453676	15.687079
24.080366	1212.679986	15.692096
23.934610	1228.785944	15.697114
23.826116	1228.789096	15.702131
23.832042	1216.206245	15.707149
24.078646	1232.288699	15.712167
24.181143	1241.339207	15.717184
24.518127	1253.825620	15.722202
24.444381	1260.673136	15.727219
24.894767	1241.701074	15.732237
24.659112	1224.626572	15.737255
24.413354	1218.714574	15.742272
24.315680	1215.881548	15.747290
24.388217	1215.457405	15.752307
24.598665	1213.909271	15.757325
24.423815	1222.419475	15.762343
24.343246	1215.361066	15.767360
24.380856	1211.553277	15.772378
24.673256	1223.804356	15.777395
24.422639	1209.781662	15.782413
24.356338	1238.684463	15.787431
24.565242	1252.236561	15.792448
24.677275	1244.925479	15.797466
24.751932	1245.596679	15.802483
24.811553	1243.689865	15.807501
24.437843	1241.995192	15.812519
24.683201	1244.654597	15.817536
24.990375	1246.483837	15.822554
24.847203	1248.784878	15.827571
24.965741	1245.176862	15.832589
24.586285	1254.900041	15.837607
24.595219	1247.488494	15.842624
24.708340	1239.645232	15.847642
24.787737	1246.373157	15.852659
24.991345	1241.790801	15.857677
24.435512	1257.489829	15.862695
24.499643	1256.404187	15.867712
24.755044	1247.834959	15.872730
24.717543	1266.757070	15.877747
25.262973	1275.243729	15.882765
24.653860	1282.984720	15.887783
25.260281	1279.608620	15.892800
25.122934	1276.753797	15.897818
24.902157	1283.391798	15.902835
25.413139	1269.108172	15.907853
25.260511	1274.570523	15.912871
25.703808	1273.361009	15.917888
25.513871	1276.495638	15.922906
25.243457	1272.369110	15.927923
25.505809	1262.998259	15.932941
25.219334	1245.247004	15.937959
25.279026	1255.832110	15.942976
25.163986	1249.961283	15.947994
25.259060	1258.297983	15.953011
25.683785	1260.983055	15.958029
25.521914	1268.488344	15.963047
25.577618	1264.859019	15.968064
25.639298	1264.617941	15.973082
25.420206	1269.021559	15.978099
25.571881	1264.811305	15.983117
25.699358	1279.240725	15.988135
25.643647	1262.909749	15.993152
25.803295	1267.353713	15.998170
25.490032	1277.587343	16.003187
25.780590	1266.473517	16.008205
25.973272	1266.802626	16.013223
25.555589	1261.390209	16.018240
25.502919	1259.591897	16.023258
25.481018	1260.301493	16.028275
25.722843	1264.009155	16.033293
25.628742	1265.170573	16.038311
25.698531	1257.427558	16.043328
25.834725	1265.508294	16.048346
25.806225	1261.860803	16.053363
25.833055	1248.707631	16.058381
25.630609	1263.777293	16.063399
25.807070	1264.918405	16.068416
25.837553	1257.554662	16.073434
25.792924	1268.455001	16.078451
26.318581	1275.005467	16.083469
26.286158	1272.993998	16.088487
26.113963	1270.939495	16.093504
25.964120	1268.674049	16.098522
25.853891	1270.026883	16.103539
26.319860	1274.821937	16.108557
26.303058	1290.932827	16.113575
25.849519	1302.204064	16.118592
26.405162	1301.283218	16.123610
26.170496	1302.963856	16.128627
26.181404	1289.850873	16.133645
26.606854	1304.200173	16.138663
26.262685	1301.923731	16.143680
26.485163	1300.972917	16.148698
26.301037	1301.203101	16.153715
26.741056	1289.491419	16.158733
26.013752	1296.543397	16.163751
26.299344	1291.199366	16.168768
26.333925	1296.448926	16.173786
26.050320	1302.417108	16.178803
26.465170	1299.969769	16.183821
26.241837	1294.368947	16.188839
26.210737	1289.076465	16.193856
26.471085	1302.842119	16.198874
26.402742	1319.048157	16.203891
26.160274	1324.255728	16.208909
26.590734	1323.040459	16.213927
26.692772	1316.359836	16.218944
27.235751	1322.189262	16.223962
26.674257	1322.050380	16.228979
26.822741	1314.860583	16.233997
27.087571	1327.418617	16.239015
27.142060	1313.190510	16.244032
27.587526	1318.111979	16.249050
26.986713	1314.700765	16.254067
26.964100	1302.451053	16.259085
27.033686	1290.711231	16.264103
26.687855	1289.994863	16.269120
27.288737	1297.095025	16.274138
26.975646	1307.065104	16.279155
27.142827	1301.532599	16.284173
27.189867	1314.381889	16.289191
26.907385	1318.967427	16.294208
27.232423	1318.298830	16.299226
27.503685	1314.412645	16.304243
27.538776	1315.221273	16.309261
27.244846	1285.471077	16.314279
27.168285	1289.405153	16.319296
27.387501	1289.728697	16.324314
26.897421	1282.032332	16.329331
27.435000	1297.959896	16.334349
27.246626	1311.962680	16.339367
27.163824	1319.610415	16.344384
27.582807	1319.517541	16.349402
27.507929	1318.509780	16.354419
27.235009	1318.494835	16.359437
27.428392	1311.065176	16.364455
27.373016	1321.819910	16.369472
27.720372	1313.655268	16.374490
27.244552	1310.988636	16.379507
27.482548	1318.428852	16.384525
27.488812	1312.670022	16.389543
27.100829	1318.716277	16.394560
27.202656	1312.675553	16.399578
27.512558	1324.892133	16.404595
27.967624	1341.907033	16.409613
27.925702	1344.877473	16.414631
27.753867	1338.445809	16.419648
27.938864	1348.668787	16.424666
27.767656	1353.888801	16.429683
27.902606	1347.746738	16.434701
28.216657	1349.691175	16.439719
27.719034	1347.678042	16.444736
27.999980	1345.072142	16.449754
28.168860	1342.390682	16.454771
28.065295	1344.810370	16.459789
28.106546	1344.260312	16.464807
27.894087	1347.223311	16.469824
27.956901	1346.699212	16.474842
27.949078	1348.407908	16.479859
27.750181	1335.288423	16.484877
27.948915	1349.261515	16.489895
27.834929	1340.035671	16.494912
27.941344	1341.400734	16.499930
27.825536	1346.261053	16.504947
27.986961	1355.035001	16.509965
28.074465	1366.708927	16.514983
28.014946	1370.659495	16.520000
28.425077	1367.074906	16.525018
28.136012	1374.772303	16.530035
28.418070	1362.028364	16.535053
28.521712	1367.435014	16.540071
28.607026	1371.421875	16.545088
28.407995	1363.925760	16.550106
28.386852	1363.008116	16.555123
28.555641	1368.439231	16.560141
28.905930	1374.817177	16.565159
28.581914	1363.691277	16.570176
28.654889	1368.508596	16.575194
28.614922	1374.258224	16.580211
28.823179	1371.572023	16.585229
29.049376	1367.861751	16.590247
28.733263	1369.484803	16.595264
29.040542	1371.165638	16.600282
29.004644	1361.657822	16.605299
28.616697	1366.368267	16.610317
29.123113	1360.295501	16.615335
28.881535	1371.645130	16.620352
28.853756	1361.162103	16.625370
28.739284	1367.826464	16.630387
28.993161	1362.370935	16.635405
29.146084	1357.390487	16.640423
28.929347	1365.077698	16.645440
28.897014	1367.076821	16.650458
28.674731	1372.003949	16.655475
28.986962	1361.714104	16.660493
29.092800	1357.253959	16.665511
28.778865	1365.148543	16.670528
29.239285	1371.980854	16.675546
29.363112	1396.252039	16.680563
29.078883	1401.883011	16.685581
29.417904	1394.071620	16.690599
28.903826	1402.787763	16.695616
29.144020	1393.342357	16.700634
29.381959	1398.799452	16.705651
29.149204	1397.738850	16.710669
29.410730	1398.560448	16.715687
29.136059	1393.696707	16.720704
29.391390	1394.174497	16.725722
29.341165	1393.933606	16.730739
29.158889	1394.866334	16.735757
29.548177	1404.044322	16.740775
29.810169	1416.601914	16.745792
29.902068	1414.759814	16.750810
29.784757	1398.927384	16.755827
29.444510	1393.090767	16.760845
29.693090	1395.026938	16.765863
29.825223	1414.208752	16.770880
29.866618	1410.889193	16.775898
29.631111	1412.083832	16.780915
29.608963	1417.312891	16.785933
29.603433	1411.399302	16.790951
29.799558	1407.156865	16.795968
30.367525	1413.900960	16.800986
30.215367	1416.094275	16.806003
30.243266	1410.253301	16.811021
30.448937	1413.719963	16.816039
30.189419	1404.398661	16.821056
29.923026	1391.456595	16.826074
30.177670	1394.573872	16.831091
29.906293	1409.281303	16.836109
30.052349	1402.104858	16.841127
29.979691	1405.068382	16.846144
30.292408	1403.298241	16.851162
30.438141	1404.428893	16.856179
30.401565	1411.579145	16.861197
30.323000	1404.033383	16.866215
30.241157	1410.863605	16.871232
30.362936	1405.380686	16.876250
30.424468	1407.279866	16.881267
30.542342	1405.479136	16.886285
30.534529	1400.474063	16.891303
30.869789	1410.167208	16.896320
30.783106	1400.564429	16.901338
30.427609	1393.108131	16.906355
30.327834	1396.802406	16.911373
30.404065	1391.903311	16.916391
30.284388	1408.525542	16.921408
30.195192	1394.755489	16.926426
30.727138	1407.907935	16.931443
30.458168	1407.004673	16.936461
30.813479	1403.066787	16.941479
30.322126	1406.216022	16.946496
30.417050	1395.325350	16.951514
30.740292	1413.178923	16.956531
30.831483	1431.390700	16.961549
31.120848	1438.367040	16.966567
31.275580	1440.377772	16.971584
31.045631	1410.976354	16.976602
31.231788	1400.146771	16.981619
30.954901	1402.145374	16.986637
31.209607	1397.195527	16.991655
30.949340	1402.723341	16.996672
30.746176	1394.309525	17.001690
31.292435	1420.230173	17.006707
31.288432	1427.954099	17.011725
31.291469	1417.515147	17.016743
31.049641	1436.578303	17.021760
31.283330	1430.930839	17.026778
31.585811	1428.882309	17.031795
31.327337	1438.551756	17.036813
31.742848	1430.176803	17.041831
31.338967	1419.303789	17.046848
31.352844	1401.371832	17.051866
31.412642	1404.623067	17.056883
31.357907	1419.030376	17.061901
31.555049	1425.851700	17.066919
31.448658	1432.391347	17.071936
31.354272	1428.717309	17.076954
31.821342	1442.871110	17.081971
31.395865	1437.283369	17.086989
31.869218	1421.660937	17.092007
31.839971	1426.002719	17.097024
31.530123	1429.929523	17.102042
31.923443	1426.625414	17.107059
31.468778	1424.268409	17.112077
31.593151	1425.063863	17.117095
31.617046	1430.554175	17.122112
31.559188	1432.945854	17.127130
31.939110	1419.954232	17.132147
31.789706	1434.241983	17.137165
31.718829	1435.782001	17.142183
31.507146	1435.009210	17.147200
31.730126	1457.393315	17.152218
31.907448	1448.147411	17.157235
31.986138	1462.651001	17.162253
31.880461	1464.759488	17.167271
32.043688	1459.164006	17.172288
31.748279	1462.906175	17.177306
31.958129	1452.067720	17.182323
32.098337	1479.117227	17.187341
32.488701	1476.784914	17.192359
32.460978	1489.981501	17.197376
32.569968	1475.006744	17.202394
32.606455	1455.994959	17.207411
32.279964	1466.952646	17.212429
32.593041	1451.085844	17.217447
32.547786	1444.110458	17.222464
32.382847	1450.032319	17.227482
32.614220	1436.094112	17.232499
32.433460	1456.738113	17.237517
32.642106	1460.007669	17.242535
32.908930	1479.128532	17.247552
32.850379	1463.108989	17.252570
32.535054	1453.477830	17.257587
32.477614	1467.197737	17.262605
32.662449	1473.686913	17.267623
32.462697	1482.909345	17.272640
32.709392	1488.823424	17.277658
32.851834	1482.022091	17.282675
33.008117	1486.948694	17.287693
32.712416	1486.665112	17.292711
33.092445	1494.570259	17.297728
32.838694	1476.983776	17.302746
32.931911	1484.152371	17.307763
32.919806	1483.893960	17.312781
32.928746	1481.259180	17.317799
33.145520	1485.932514	17.322816
32.936332	1474.199846	17.327834
33.292434	1481.192732	17.332851
32.888185	1485.227657	17.337869
33.133696	1483.366462	17.342887
33.115269	1489.496574	17.347904
33.276104	1496.618770	17.352922
33.448586	1503.959879	17.357939
33.371027	1508.285656	17.362957
33.520639	1506.892605	17.367975
33.757697	1507.471240	17.372992
33.586380	1491.313828	17.378010
33.856871	1484.464960	17.383027
33.323643	1479.269169	17.388045
33.139194	1470.727433	17.393063
33.836928	1494.773046	17.398080
33.670013	1498.903183	17.403098
33.772265	1494.617778	17.408115
33.699503	1498.692795	17.413133
33.936664	1503.741846	17.418151
34.235290	1494.460910	17.423168
33.974317	1490.366221	17.428186
34.006113	1468.093651	17.433203
33.738237	1480.200157	17.438221
33.688318	1466.573921	17.443239
34.212401	1468.206933	17.448256
33.747933	1483.566335	17.453274
33.975023	1478.990461	17.458291
33.749695	1500.483103	17.463309
34.219362	1495.399683	17.468327
34.200881	1496.029798	17.473344
34.018406	1495.341535	17.478362
34.330124	1490.310987	17.483379
34.083298	1505.615155	17.488397
33.871136	1496.311557	17.493415
34.067227	1493.085887	17.498432
34.133435	1500.343390	17.503450
34.410670	1487.744219	17.508467
34.229223	1485.338510	17.513485
34.183877	1493.016553	17.518503
34.406988	1491.440515	17.523520
34.034753	1494.498833	17.528538
34.274683	1491.524937	17.533555
34.424451	1518.448542	17.538573
34.471853	1524.531180	17.543591
34.637318	1524.641005	17.548608
34.844473	1525.548947	17.553626
34.745799	1518.956909	17.558643
34.804005	1532.278486	17.563661
34.869805	1515.909446	17.568679
34.778647	1523.132935	17.573696
34.681654	1523.884278	17.578714
34.726184	1518.528242	17.583731
34.847132	1531.057472	17.588749
34.492806	1521.176058	17.593767
34.978851	1517.600343	17.598784
34.601499	1524.581011	17.603802
35.031332	1523.548089	17.608819
34.793932	1525.526010	17.613837
34.961613	1529.296771	17.618855
35.299537	1524.918285	17.623872
34.938863	1529.600063	17.628890
35.179392	1526.197775	17.633907
35.187675	1518.497663	17.638925
34.937885	1519.946996	17.643943
34.884934	1529.097172	17.648960
34.806585	1548.017521	17.653978
35.278433	1547.610639	17.658995
35.180769	1555.438481	17.664013
35.237264	1559.869070	17.669031
35.744492	1536.801396	17.674048
35.491143	1549.544443	17.679066
35.561357	1549.456653	17.684083
35.632811	1542.866211	17.689101
35.410573	1542.128618	17.694119
35.445965	1549.341638	17.699136
35.602444	1548.710729	17.704154
35.437850	1543.739194	17.709171
35.847869	1556.939473	17.714189
35.466971	1568.652183	17.719207
36.244196	1566.704094	17.724224
35.963775	1566.229033	17.729242
35.839329	1561.199684	17.734259
35.997808	1564.399218	17.739277
36.002769	1559.977728	17.744295
36.297981	1561.138210	17.749312
36.335618	1554.422857	17.754330
36.273236	1547.235717	17.759347
36.332284	1546.202659	17.764365
36.341699	1539.019404	17.769383
36.225347	1535.284609	17.774400
35.989240	1535.140762	17.779418
36.390791	1539.161419	17.784435
36.330847	1526.046756	17.789453
36.137651	1539.206566	17.794471
36.487236	1525.937034	17.799488
36.523357	1533.162325	17.804506
36.491453	1534.349701	17.809523
36.429472	1519.855650	17.814541
36.266215	1533.593891	17.819559
36.385883	1526.848460	17.824576
36.058926	1543.126207	17.829594
36.267395	1542.045232	17.834611
36.247692	1560.158575	17.839629
36.430418	1574.952319	17.844647
36.853011	1560.809392	17.849664
36.606640	1561.541727	17.854682
36.810116	1559.890985	17.859699
36.814411	1562.062009	17.864717
36.654504	1565.139772	17.869735
36.829526	1561.618201	17.874752
36.553257	1577.024340	17.879770
36.920916	1569.390190	17.884787
37.001937	1572.071299	17.889805
36.873559	1584.165265	17.894823
37.103010	1585.429123	17.899840
37.462090	1587.604700	17.904858
37.290497	1583.823124	17.909875
37.231482	1567.865548	17.914893
37.120904	1564.952907	17.919911
37.512341	1562.606234	17.924928
37.127735	1566.534207	17.929946
37.137857	1563.065277	17.934963
37.171212	1583.254829	17.939981
36.950652	1593.369621	17.944999
37.383794	1583.503880	17.950016
37.149821	1589.376385	17.955034
37.126892	1581.272990	17.960051
37.018624	1578.368625	17.965069
37.017660	1595.205660	17.970087
37.023995	1595.081976	17.975104
37.248620	1609.881427	17.980122
37.784306	1620.111389	17.985139
37.897696	1615.062991	17.990157
37.376584	1615.578759	17.995175
37.859591	1615.022412	18.000192
37.831910	1611.565820	18.005210
37.428700	1617.997136	18.010227
38.231694	1615.940073	18.015245
38.080079	1616.979937	18.020263
38.168004	1611.594259	18.025280
38.037473	1618.015942	18.030298
37.947033	1613.302173	18.035315
38.220532	1613.709459	18.040333
38.244753	1612.805954	18.045351
38.072387	1609.715746	18.050368
37.947093	1613.306036	18.055386
38.208608	1600.446413	18.060403
38.097734	1612.336158	18.065421
38.035129	1619.204233	18.070439
38.324316	1629.978610	18.075456
38.627587	1643.021823	18.080474
38.573409	1639.194653	18.085491
38.730912	1635.582666	18.090509
38.747969	1635.324156	18.095527
38.877134	1617.063488	18.100544
38.525851	1605.907867	18.105562
38.444343	1609.993215	18.110579
38.801815	1600.731031	18.115597
38.503899	1610.966674	18.120615
38.971032	1619.790438	18.125632
38.821341	1616.160332	18.130650
38.585287	1612.741717	18.135667
38.815287	1627.055125	18.140685
38.648677	1631.992817	18.145703
39.230995	1625.969405	18.150720
39.250381	1632.870584	18.155738
39.007600	1627.679493	18.160755
39.595175	1625.975898	18.165773
38.789657	1623.042674	18.170791
39.227314	1610.967802	18.175808
39.447270	1627.262723	18.180826
39.145191	1620.514516	18.185843
39.324105	1608.707965	18.190861
39.039862	1614.016225	18.195879
38.950995	1616.011339	18.200896
39.212105	1633.277288	18.205914
39.299171	1625.365507	18.210931
39.407905	1626.894560	18.215949
39.519546	1629.444061	18.220967
39.523324	1623.144849	18.225984
39.350019	1627.058782	18.231002
39.222764	1622.134194	18.236019
39.416783	1632.265135	18.241037
39.119158	1629.455431	18.246055
39.280394	1638.692504	18.251072
39.432390	1655.547235	18.256090
39.517142	1657.203467	18.261107
39.805054	1651.249363	18.266125
39.484173	1662.619200	18.271143
39.942673	1662.834715	18.276160
39.845914	1651.742104	18.281178
39.720362	1656.838942	18.286195
39.915838	1642.749218	18.291213
39.683073	1654.762472	18.296231
39.821354	1655.071844	18.301248
39.990070	1661.269904	18.306266
39.992033	1673.672869	18.311283
40.158955	1676.209109	18.316301
40.322404	1684.325910	18.321319
40.244242	1688.922668	18.326336
40.815373	1674.176623	18.331354
40.172239	1675.637042	18.336371
40.624018	1682.848235	18.341389
40.298177	1684.822684	18.346407
40.447453	1679.799237	18.351424
40.739284	1677.959888	18.356442
40.425838	1683.325746	18.361459
41.145373	1674.227082	18.366477
41.086190	1681.012346	18.371495
40.892396	1664.603381	18.376512
40.624930	1653.421868	18.381530
40.630718	1658.753268	18.386547
40.751110	1663.197734	18.391565
40.867431	1670.460617	18.396583
40.795883	1671.736237	18.401600
40.789723	1668.531160	18.406618
40.758101	1677.424979	18.411635
40.616522	1669.956222	18.416653
40.641685	1673.686405	18.421671
40.785720	1662.089882	18.426688
40.641731	1668.958437	18.431706
40.428915	1690.623664	18.436723
40.880057	1690.665221	18.441741
41.133828	1709.645241	18.446759
40.953843	1705.970126	18.451776
41.361758	1713.287389	18.456794
41.170196	1707.532956	18.461811
41.223506	1699.722175	18.466829
40.969000	1712.610608	18.471847
41.498814	1718.197710	18.476864
41.551337	1727.531335	18.481882
41.749108	1735.650561	18.486899
41.822859	1733.239644	18.491917
41.792878	1730.872834	18.496935
41.974773	1731.781618	18.501952
41.916711	1728.575264	18.506970
41.746709	1721.737478	18.511987
42.265949	1705.861342	18.517005
41.794871	1698.501149	18.522023
41.835135	1690.677964	18.527040
41.998354	1698.667859	18.532058
41.819545	1707.407105	18.537075
42.228742	1720.122289	18.542093
42.371687	1722.780201	18.547111
42.059651	1717.232067	18.552128
41.917418	1713.303302	18.557146
42.000832	1723.210486	18.562163
42.232174	1716.676017	18.567181
42.421095	1729.112690	18.572199
42.060052	1724.439078	18.577216
42.445103	1723.649932	18.582234
42.154553	1728.777604	18.587251
42.545779	1728.522606	18.592269
42.283218	1721.230490	18.597287
42.418930	1723.840784	18.602304
42.766580	1725.006785	18.607322
42.747533	1720.271737	18.612339
42.768690	1720.820321	18.617357
42.810777	1720.604124	18.622375
42.588283	1725.504040	18.627392
42.668661	1719.273419	18.632410
42.538315	1717.273743	18.637427
42.645028	1720.273819	18.642445
42.565024	1716.972288	18.647463
42.484916	1722.760565	18.652480
42.655010	1729.746711	18.657498
42.766177	1743.704322	18.662515
43.308042	1738.696284	18.667533
43.256583	1750.846558	18.672551
42.900258	1750.667857	18.677568
43.308258	1739.039071	18.682586
43.119761	1740.600721	18.687603
43.184719	1743.218972	18.692621
43.314330	1743.109359	18.697639
43.241360	1750.844648	18.702656
43.642706	1740.524670	18.707674
43.181456	1746.342875	18.712691
43.516437	1742.619261	18.717709
43.222311	1744.547733	18.722727
43.303707	1740.443834	18.727744
43.655877	1734.923315	18.732762
43.263647	1746.234146	18.737779
43.537514	1752.317634	18.742797
43.507896	1760.089459	18.747815
43.701867	1769.980568	18.752832
43.794774	1768.536439	18.757850
43.685948	1773.810254	18.762867
43.912496	1778.051013	18.767885
43.907810	1764.477464	18.772903
43.984479	1761.156330	18.777920
44.094115	1765.311695	18.782938
43.921062	1771.867225	18.787955
44.150414	1757.185060	18.792973
43.931522	1768.588311	18.797991
44.249853	1770.951532	18.803008
44.227128	1753.922149	18.808026
43.959344	1770.173429	18.813043
44.196755	1790.019531	18.818061
44.575353	1793.431329	18.823079
44.531797	1803.976204	18.828096
44.781021	1792.684995	18.833114
44.606378	1797.501641	18.838131
44.758224	1801.192222	18.843149
44.890875	1797.915366	18.848167
44.703011	1780.170617	18.853184
44.884181	1771.335055	18.858202
44.750511	1774.848036	18.863219
44.721396	1766.224173	18.868237
44.978811	1765.971605	18.873255
44.675055	1782.646311	18.878272
44.895460	1790.615387	18.883290
44.976987	1792.216465	18.888307
45.166621	1786.349211	18.893325
44.910570	1789.127591	18.898343
44.798127	1789.351250	18.903360
45.070585	1781.143628	18.908378
44.946307	1796.427242	18.913395
44.785295	1785.215444	18.918413
44.925717	1791.540264	18.923431
45.049360	1786.596599	18.928448
45.229976	1796.149030	18.933466
45.250749	1813.551934	18.938483
45.349482	1812.692199	18.943501
45.398603	1818.249536	18.948519
45.346948	1817.455988	18.953536
45.659356	1812.208319	18.958554
45.677983	1813.240927	18.963571
45.690537	1813.107750	18.968589
45.641173	1818.413874	18.973607
45.401948	1810.532300	18.978624
45.779135	1807.313445	18.983642
45.766852	1813.703859	18.988659
45.751178	1803.378157	18.993677
45.646014	1804.537113	18.998695
45.494181	1818.978753	19.003712
45.763663	1833.625552	19.008730
45.933030	1838.527471	19.013747
46.060155	1842.347329	19.018765
46.261582	1837.757088	19.023783
46.438202	1842.995565	19.028800
46.437096	1830.856629	19.033818
46.459700	1833.041986	19.038835
46.671522	1828.655518	19.043853
46.895324	1820.312625	19.048871
46.693509	1828.329253	19.053888
46.803519	1811.661290	19.058906
46.950404	1800.538740	19.063923
46.759933	1788.815335	19.068941
46.842046	1787.776088	19.073959
46.596877	1783.793458	19.078976
46.831700	1776.618899	19.083994
46.995880	1783.001004	19.089011
46.880857	1779.314152	19.094029
46.952855	1766.960453	19.099047
46.940163	1786.255041	19.104064
47.083039	1774.186241	19.109082
46.724236	1784.928260	19.114099
46.744471	1782.089422	19.119117
46.613391	1784.707205	19.124135
46.813745	1804.235473	19.129152
47.112499	1811.702303	19.134170
47.090322	1826.544716	19.139187
47.023594	1814.768563	19.144205
47.170050	1816.738789	19.149223
47.017026	1828.198317	19.154240
47.173248	1812.179724	19.159258
47.281648	1820.604084	19.164275
47.534500	1838.119630	19.169293
48.021302	1839.035703	19.174311
47.441903	1842.790842	19.179328
48.021559	1832.710990	19.184346
48.104235	1832.573507	19.189363
47.491322	1827.606486	19.194381
47.957614	1823.385423	19.199399
47.704302	1844.660362	19.204416
47.873217	1834.936145	19.209434
48.089825	1843.558752	19.214451
47.835951	1832.821856	19.219469
47.815748	1837.175053	19.224487
47.612133	1839.781804	19.229504
47.703395	1834.611022	19.234522
47.884232	1842.874819	19.239539
48.136551	1839.982658	19.244557
48.268652	1840.573141	19.249575
48.241151	1843.380880	19.254592
48.468865	1850.650831	19.259610
48.325848	1859.548205	19.264627
48.314095	1869.602888	19.269645
48.597139	1867.536453	19.274663
48.590317	1880.967491	19.279680
48.784451	1873.074106	19.284698
48.746900	1879.303782	19.289715
48.711648	1865.620444	19.294733
48.865018	1872.590327	19.299751
48.382496	1870.577775	19.304768
48.262288	1867.408036	19.309786
48.544671	1874.957317	19.314803
48.483268	1873.777824	19.319821
48.604875	1873.518763	19.324839
48.513100	1871.935281	19.329856
48.706996	1883.865215	19.334874
48.631692	1899.440016	19.339891
48.778558	1897.919052	19.344909
49.263990	1893.418461	19.349927
49.363551	1904.707973	19.354944
49.426197	1901.899304	19.359962
49.347494	1893.748865	19.364979
49.371244	1902.973586	19.369997
49.470234	1893.114842	19.375015
49.500909	1902.215597	19.380032
49.425502	1891.623950	19.385050
49.431744	1896.587487	19.390067
49.520560	1912.990790	19.395085
50.009640	1906.316416	19.400103
49.614075	1911.490829	19.405120
49.854475	1913.260918	19.410138
49.888188	1919.034987	19.415155
49.783587	1922.367233	19.420173
50.028787	1913.356263	19.425191
50.030743	1910.935532	19.430208
50.182652	1909.911708	19.435226
50.204177	1911.179446	19.440243
50.215819	1920.085545	19.445261
50.419026	1912.485686	19.450279
50.336443	1921.541396	19.455296
50.228010	1917.757173	19.460314
50.323307	1909.346108	19.465331
50.478123	1916.362223	19.470349
50.578481	1911.449725	19.475367
50.575027	1907.175376	19.480384
50.679615	1911.806560	19.485402
50.634988	1901.319257	19.490419
50.476023	1916.192431	19.495437
50.736280	1906.222393	19.500455
50.668770	1910.147061	19.505472
50.945373	1909.869276	19.510490
50.553902	1914.263181	19.515507
50.425656	1912.899871	19.520525
50.511661	1915.538292	19.525543
50.624517	1924.232414	19.530560
50.654869	1925.208964	19.535578
50.791323	1928.937745	19.540595
50.914990	1934.334593	19.545613
50.754919	1927.271871	19.550631
50.870764	1944.838916	19.555648
51.147554	1953.850414	19.560666
51.545532	1956.636872	19.565683
51.917663	1951.687520	19.570701
51.796783	1963.410703	19.575719
51.440421	1959.751093	19.580736
51.565131	1952.081518	19.585754
51.894739	1955.885855	19.590771
51.332191	1958.498206	19.595789
51.453425	1942.057355	19.600807
51.663387	1948.951393	19.605824
51.880097	1948.971464	19.610842
52.154816	1942.937942	19.615859
51.731360	1954.789852	19.620877
51.825070	1950.060901	19.625895
51.899848	1954.236642	19.630912
52.045446	1949.217061	19.635930
52.143929	1942.362365	19.640947
51.995147	1951.055255	19.645965
52.209789	1950.221433	19.650983
52.409636	1951.384911	19.656000
51.884753	1946.859158	19.661018
52.438457	1949.480329	19.666035
52.202781	1945.620287	19.671053
52.507404	1951.387587	19.676071
52.611660	1973.913508	19.681088
52.494445	1982.316978	19.686106
52.910030	1970.077186	19.691123
52.517899	1986.309482	19.696141
52.447973	1984.959951	19.701159
52.820827	1980.513565	19.706176
52.861165	1981.195193	19.711194
52.822715	1977.620232	19.716211
52.517994	1979.942763	19.721229
52.680517	1980.228848	19.726247
52.728666	1978.967470	19.731264
52.951921	1978.325509	19.736282
52.935512	1981.555802	19.741299
53.148655	2006.924487	19.746317
53.137803	2006.360381	19.751335
53.338659	2015.408672	19.756352
53.214811	2020.142199	19.761370
53.708081	2007.773607	19.766387
53.418404	2019.525121	19.771405
53.684908	2009.031206	19.776423
53.728929	2009.238656	19.781440
53.620945	2010.036125	19.786458
53.809791	2002.026829	19.791475
53.742092	2015.328099	19.796493
53.859826	2003.713620	19.801511
53.904431	1994.262968	19.806528
53.724253	2005.376956	19.811546
53.855127	2006.877195	19.816563
53.676670	2003.100586	19.821581
53.666499	2010.437874	19.826599
53.845075	2014.479956	19.831616
53.923923	2025.889897	19.836634
53.836243	2034.211358	19.841651
53.851097	2035.218622	19.846669
53.570782	2044.748962	19.851687
54.049856	2036.023058	19.856704
54.093901	2063.474088	19.861722
54.661269	2056.252320	19.866739
54.742027	2068.438273	19.871757
54.526572	2066.158552	19.876775
54.726997	2060.388417	19.881792
54.539234	2061.937381	19.886810
55.045306	2062.400922	19.891827
54.998271	2053.805250	19.896845
54.887303	2060.239631	19.901863
54.920514	2047.632696	19.906880
54.812923	2056.287543	19.911898
55.072406	2048.458655	19.916915
54.877194	2053.156352	19.921933
55.090312	2052.085400	19.926951
55.287787	2056.687893	19.931968
54.819835	2054.587287	19.936986
55.049762	2057.401141	19.942003
54.954113	2074.125423	19.947021
55.321027	2077.887802	19.952039
55.410968	2081.585334	19.957056
55.404724	2097.490423	19.962074
55.604696	2087.303483	19.967091
55.424744	2088.501391	19.972109
55.672272	2090.012870	19.977127
55.632736	2081.860189	19.982144
55.495238	2089.724409	19.987162
55.570298	2072.896209	19.992179
55.578798	2084.170195	19.997197
55.986032	2109.639638	20.002215
56.088991	2111.958985	20.007232
55.802369	2116.843049	20.012250
56.307979	2122.958264	20.017267
56.260027	2114.155251	20.022285
56.055371	2112.900603	20.027303
56.182351	2107.539397	20.032320
56.141828	2116.993742	20.037338
56.526886	2103.800128	20.042355
56.522835	2112.393215	20.047373
56.366986	2109.614120	20.052391
56.918279	2099.160672	20.057408
56.594184	2106.419384	20.062426
56.758901	2101.153706	20.067443
56.661665	2095.714017	20.072461
56.553473	2099.535625	20.077479
56.580010	2098.795275	20.082496
56.804595	2107.154731	20.087514
56.863380	2107.487092	20.092531
56.840139	2106.231399	20.097549
56.856816	2120.908636	20.102567
57.255244	2114.898301	20.107584
57.038516	2136.398478	20.112602
57.111334	2126.796050	20.117619
57.277719	2132.405572	20.122637
57.008712	2128.782661	20.127655
57.336458	2128.563541	20.132672
56.982179	2130.663991	20.137690
57.286555	2121.024876	20.142707
57.653893	2133.406412	20.147725
57.441201	2154.374700	20.152743
57.720008	2150.296529	20.157760
57.960396	2154.974433	20.162778
58.272969	2150.307865	20.167795
58.135227	2152.157006	20.172813
57.811003	2147.483674	20.177831
58.381820	2134.894313	20.182848
58.408005	2135.327131	20.187866
58.315589	2121.623881	20.192883
58.362328	2124.096601	20.197901
57.956094	2119.564179	20.202919
58.284026	2103.910570	20.207936
57.805431	2123.665405	20.212954
58.142473	2135.208136	20.217971
58.111977	2140.955894	20.222989
58.357315	2154.886589	20.228007
58.546712	2150.037838	20.233024
58.639213	2160.866743	20.238042
58.627891	2149.528377	20.243059
58.485707	2147.578037	20.248077
58.160980	2155.151806	20.253095
58.515306	2166.990690	20.258112
58.404236	2180.754737	20.263130
58.864254	2178.108086	20.268147
58.985464	2188.193755	20.273165
58.708848	2188.438446	20.278183
59.108485	2175.655708	20.283200
58.632750	2194.584258	20.288218
59.300544	2200.341239	20.293235
59.421144	2204.172697	20.298253
59.117750	2209.413268	20.303271
59.613659	2204.875427	20.308288
59.507803	2204.836217	20.313306
59.614581	2201.691295	20.318323
60.004889	2202.249752	20.323341
59.924825	2205.089272	20.328359
60.011068	2196.045356	20.333376
59.516068	2215.603433	20.338394
59.817969	2202.224481	20.343411
60.232030	2203.645662	20.348429
59.771923	2208.144289	20.353447
60.019516	2199.676013	20.358464
59.609107	2203.217108	20.363482
60.065521	2198.218518	20.368499
59.997102	2198.888013	20.373517
59.769512	2203.179924	20.378535
60.033524	2193.445082	20.383552
59.905770	2209.833905	20.388570
60.088259	2216.891052	20.393587
60.552805	2219.196131	20.398605
60.186184	2230.573942	20.403623
60.619520	2221.458678	20.408640
60.506705	2221.910335	20.413658
60.459757	2220.678431	20.418675
60.622025	2218.809845	20.423693
60.595290	2239.917582	20.428711
60.882588	2237.021537	20.433728
60.973684	2249.820434	20.438746
61.196303	2255.583685	20.443763
61.185979	2247.677444	20.448781
61.159954	2251.437287	20.453799
61.581250	2245.412494	20.458816
61.667562	2253.814957	20.463834
61.113878	2242.468717	20.468851
61.077129	2243.492986	20.473869
61.216708	2242.978218	20.478887
61.500724	2240.906653	20.483904
61.392652	2246.457054	20.488922
61.610276	2239.527424	20.493939
61.455062	2237.533954	20.498957
61.422502	2246.727638	20.503975
61.660720	2266.825576	20.508992
61.929724	2271.229324	20.514010
61.868663	2261.387740	20.519027
62.242987	2263.996881	20.524045
62.154673	2270.079803	20.529063
62.290315	2268.353393	20.534080
62.348671	2259.766369	20.539098
62.305207	2255.328866	20.544115
62.449476	2258.080542	20.549133
62.340256	2257.231528	20.554151
62.800690	2257.639829	20.559168
62.686328	2255.329399	20.564186
62.482694	2260.171253	20.569203
62.806990	2254.826204	20.574221
62.574714	2263.818671	20.579239
62.797128	2262.396791	20.584256
62.850723	2264.853638	20.589274
62.494317	2269.360537	20.594291
62.490699	2262.621972	20.599309
62.679552	2261.157218	20.604327
62.738114	2275.551918	20.609344
62.872355	2291.741051	20.614362
62.646775	2285.324365	20.619379
63.001699	2289.571216	20.624397
62.902442	2303.618630	20.629415
63.139466	2292.825092	20.634432
63.111527	2309.693347	20.639450
63.236758	2306.830566	20.644467
63.528160	2304.741829	20.649485
63.232237	2319.232351	20.654503
63.201267	2302.882994	20.659520
63.628135	2316.342539	20.664538
63.555238	2311.032008	20.669555
63.969041	2325.303490	20.674573
63.622337	2323.721737	20.679591
64.030692	2335.239646	20.684608
64.286468	2333.367404	20.689626
64.041896	2336.898249	20.694643
64.411878	2333.011244	20.699661
64.110809	2336.310698	20.704679
64.283271	2341.017795	20.709696
64.431879	2331.453893	20.714714
64.461199	2335.272912	20.719731
64.641732	2331.262110	20.724749
64.378325	2332.378166	20.729767
64.862785	2340.265118	20.734784
64.590982	2336.394806	20.739802
64.469214	2338.123031	20.744819
64.654577	2330.304085	20.749837
64.493096	2338.121809	20.754855
64.803047	2350.208305	20.759872
65.490334	2346.569624	20.764890
65.223644	2354.572443	20.769907
65.443338	2351.055713	20.774925
65.280949	2339.507153	20.779943
64.875808	2337.600636	20.784960
65.233292	2347.547373	20.789978
65.134056	2355.020596	20.794995
65.488212	2352.939591	20.800013
65.603960	2348.176170	20.805031
65.377787	2353.180622	20.810048
65.584044	2354.387361	20.815066
65.526404	2355.314311	20.820083
65.626786	2344.954108	20.825101
65.827153	2356.840627	20.830119
65.947314	2376.979279	20.835136
65.994388	2374.958268	20.840154
66.098351	2377.201315	20.845171
66.358543	2379.331938	20.850189
66.253030	2377.169817	20.855207
65.957213	2385.270568	20.860224
66.413731	2383.171463	20.865242
66.251683	2386.899294	20.870259
66.928743	2380.417061	20.875277
66.251329	2373.044579	20.880295
66.497888	2376.207289	20.885312
66.793518	2367.881364	20.890330
66.335986	2370.046345	20.895347
66.543825	2369.016596	20.900365
66.629990	2381.157025	20.905383
67.128843	2401.387645	20.910400
66.832029	2400.945183	20.915418
66.940807	2405.465990	20.920435
67.134414	2410.366252	20.925453
66.890538	2397.519410	20.930471
66.754449	2404.991464	20.935488
66.967339	2407.318475	20.940506
67.072422	2411.056495	20.945523
67.354175	2416.417744	20.950541
67.339612	2429.132881	20.955559
67.559176	2426.934159	20.960576
67.725609	2438.706869	20.965594
67.505874	2432.836947	20.970611
67.860371	2424.024925	20.975629
67.951088	2419.217394	20.980647
67.985367	2416.002330	20.985664
68.066834	2415.797922	20.990682
68.023397	2425.515514	20.995699
68.045723	2422.224281	21.000717
68.071594	2425.207739	21.005735
68.076785	2420.277148	21.010752
68.500362	2425.818884	21.015770
68.011110	2423.229462	21.020787
68.186420	2422.989666	21.025805
68.567433	2442.447358	21.030823
68.497080	2452.264289	21.035840
68.768688	2446.515710	21.040858
68.509912	2454.806423	21.045875
68.871779	2446.157331	21.050893
68.886385	2454.882161	21.055911
68.953804	2441.501005	21.060928
68.998208	2448.154537	21.065946
68.953228	2453.829220	21.070963
68.740070	2449.797035	21.075981
69.255564	2444.026263	21.080999
68.902435	2446.580269	21.086016
69.529558	2440.151930	21.091034
69.155830	2447.591823	21.096051
69.225192	2464.929760	21.101069
69.456856	2470.884299	21.106087
69.214201	2465.755693	21.111104
69.583842	2470.858165	21.116122
69.362272	2466.487826	21.121139
69.427410	2473.633376	21.126157
69.330996	2476.190039	21.131175
69.571152	2497.517981	21.136192
69.812804	2503.176810	21.141210
69.564161	2500.419473	21.146227
69.953956	2505.458986	21.151245
70.190055	2517.618837	21.156263
70.168013	2517.096716	21.161280
70.215626	2529.894961	21.166298
70.400039	2527.992563	21.171315
70.469394	2522.847217	21.176333
70.846758	2518.006460	21.181351
70.929211	2509.768242	21.186368
71.136343	2516.520100	21.191386
71.213994	2517.950647	21.196403
70.895836	2521.119115	21.201421
71.034608	2519.606121	21.206439
71.052722	2519.984383	21.211456
71.634395	2513.508016	21.216474
71.184533	2507.861906	21.221491
71.194863	2515.566491	21.226509
71.306671	2506.087887	21.231527
71.299065	2508.263176	21.236544
71.448881	2505.013254	21.241562
71.182590	2520.854279	21.246579
70.959278	2519.918600	21.251597
70.823045	2517.870189	21.256615
71.155754	2547.186047	21.261632
71.425382	2537.902981	21.266650
71.473985	2553.510914	21.271667
71.372589	2561.540262	21.276685
71.890513	2559.280210	21.281703
71.560580	2581.084927	21.286720
72.113132	2573.105188	21.291738
72.090793	2568.723351	21.296755
71.908854	2578.329881	21.301773
72.489904	2581.898153	21.306791
72.396434	2585.097019	21.311808
72.658413	2600.807723	21.316826
72.842903	2598.472656	21.321843
72.671171	2585.591887	21.326861
72.993159	2580.262069	21.331879
72.582340	2581.346207	21.336896
72.842556	2575.797873	21.341914
72.899780	2598.606672	21.346931
72.561723	2595.384599	21.351949
72.628582	2594.660002	21.356967
73.160526	2587.275549	21.361984
73.509732	2595.433194	21.367002
73.098204	2588.335939	21.372019
73.425388	2588.057462	21.377037
73.502411	2595.866806	21.382055
73.446129	2587.871142	21.387072
73.645210	2584.808127	21.392090
73.514780	2594.864588	21.397107
73.522200	2591.982839	21.402125
73.638262	2604.619059	21.407143
73.371224	2617.757345	21.412160
73.738156	2620.277816	21.417178
73.808318	2627.632435	21.422195
73.691983	2620.800733	21.427213
74.030431	2618.774255	21.432231
73.789432	2635.695198	21.437248
74.547181	2636.396681	21.442266
74.413121	2640.784666	21.447283
74.354004	2645.220304	21.452301
74.780016	2648.532735	21.457319
74.826763	2647.648281	21.462336
74.956544	2644.765002	21.467354
75.020751	2645.827926	21.472371
74.961762	2641.134036	21.477389
75.202255	2645.849472	21.482407
74.985666	2646.525165	21.487424
75.070875	2636.666257	21.492442
75.113475	2646.853203	21.497459
75.250306	2639.031295	21.502477
75.182438	2637.900642	21.507495
75.213552	2645.545562	21.512512
75.183143	2640.947139	21.517530
75.091530	2647.551782	21.522547
75.305197	2653.983941	21.527565
75.369598	2665.441030	21.532583
75.239710	2667.655445	21.537600
75.270606	2671.323706	21.542618
75.537992	2669.754407	21.547635
75.791202	2687.909993	21.552653
75.697238	2699.672197	21.557671
75.459489	2699.222326	21.562688
76.172659	2686.107455	21.567706
76.201472	2699.154797	21.572723
76.172703	2696.219762	21.577741
76.274312	2702.198047	21.582759
76.333095	2724.561526	21.587776
76.467297	2715.459385	21.592794
76.612847	2722.669710	21.597811
76.727269	2723.595019	21.602829
76.920910	2722.877810	21.607847
76.799878	2719.489935	21.612864
77.221162	2724.390271	21.617882
77.393890	2726.481069	21.622899
77.190869	2720.157712	21.627917
77.238050	2718.298636	21.632935
76.726725	2729.648758	21.637952
77.212982	2712.849543	21.642970
77.210850	2724.439120	21.647987
77.150055	2743.222215	21.653005
77.634397	2743.207316	21.658023
77.488872	2751.560176	21.663040
77.689219	2739.727176	21.668058
77.342626	2751.018204	21.673075
77.214786	2747.414925	21.678093
77.541331	2742.532303	21.683111
77.498047	2762.546705	21.688128
77.549198	2774.136568	21.693146
77.758327	2779.470775	21.698163
77.873210	2778.901217	21.703181
78.291200	2764.544581	21.708199
78.121751	2791.116098	21.713216
78.321108	2791.314031	21.718234
78.620075	2797.425872	21.723251
78.314865	2798.026851	21.728269
78.815323	2785.725348	21.733287
78.689757	2802.766171	21.738304
78.775281	2791.794576	21.743322
78.706545	2795.326780	21.748339
78.931788	2794.277200	21.753357
79.068652	2798.216742	21.758375
79.315157	2810.266056	21.763392
79.319324	2820.290184	21.768410
79.416551	2833.388930	21.773427
79.689064	2832.200440	21.778445
79.839322	2824.623057	21.783463
79.348718	2812.383736	21.788480
79.468443	2816.286354	21.793498
79.849576	2822.040159	21.798515
79.666453	2828.481664	21.803533
79.482800	2821.208660	21.808551
79.479468	2837.967919	21.813568
79.650434	2822.947758	21.818586
79.651666	2832.152740	21.823603
79.815251	2854.163673	21.828621
80.144415	2854.574789	21.833639
80.101403	2858.380695	21.838656
80.214925	2856.683465	21.843674
80.518190	2862.193080	21.848691
80.367151	2879.854305	21.853709
80.664289	2877.893279	21.858727
80.860229	2883.591887	21.863744
81.114352	2872.774256	21.868762
81.233426	2870.804074	21.873779
81.193316	2875.796056	21.878797
81.764007	2858.250487	21.883815
81.288311	2873.036769	21.888832
81.700974	2871.709375	21.893850
81.634895	2876.479676	21.898867
81.232174	2869.569998	21.903885
81.407203	2867.224055	21.908903
81.236156	2875.789456	21.913920
81.458683	2870.083476	21.918938
81.489114	2868.235811	21.923955
81.296559	2869.979139	21.928973
81.722617	2887.927667	21.933991
81.749566	2888.961924	21.939008
81.736150	2899.460245	21.944026
81.811355	2899.019280	21.949043
81.928132	2904.838847	21.954061
82.221901	2901.764257	21.959079
82.060585	2917.124977	21.964096
82.305015	2920.357046	21.969114
82.399898	2921.375749	21.974131
82.263574	2934.130909	21.979149
82.519961	2934.404455	21.984167
82.454350	2924.105349	21.989184
82.912061	2944.677718	21.994202
83.232905	2951.641083	21.999219
82.864183	2943.152993	22.004237
83.040158	2948.470691	22.009255
82.911968	2954.005969	22.014272
82.986648	2942.395539	22.019290
83.503865	2943.492872	22.024307
83.380577	2940.802531	22.029325
83.171873	2937.014942	22.034343
83.288796	2943.571078	22.039360
83.154172	2955.663408	22.044378
83.485864	2956.562670	22.049395
83.414382	2974.464388	22.054413
84.181051	2963.948986	22.059431
83.735690	2983.980118	22.064448
83.273242	2973.100915	22.069466
84.166691	2979.513787	22.074483
84.605120	2996.279742	22.079501
84.966868	2992.490389	22.084519
84.823040	2993.954430	22.089536
85.110748	2979.808487	22.094554
85.050957	2962.922078	22.099571
85.023889	2955.969576	22.104589
84.979562	2954.585021	22.109607
84.977002	2949.591371	22.114624
85.028309	2955.525708	22.119642
85.398835	2947.213868	22.124659
85.075269	2955.822626	22.129677
85.189858	2957.300652	22.134695
85.457664	2955.917665	22.139712
85.022390	2954.119389	22.144730
85.218935	2975.662472	22.149747
85.666939	2982.073761	22.154765
85.546682	2984.841328	22.159783
85.453466	2981.421634	22.164800
85.503133	2991.595041	22.169818
85.507206	2978.785282	22.174835
85.327399	2997.905661	22.179853
85.480903	3015.255310	22.184871
85.890483	3020.210428	22.189888
85.586400	3030.253348	22.194906
86.134969	3037.152351	22.199923
85.941488	3052.417343	22.204941
85.965134	3056.223305	22.209959
86.344199	3049.336714	22.214976
86.333214	3059.662308	22.219994
86.855817	3065.059376	22.225011
86.710886	3077.926308	22.230029
86.817571	3072.554345	22.235047
87.356857	3069.590327	22.240064
87.390583	3076.633477	22.245082
87.512048	3068.972153	22.250099
87.326257	3073.063112	22.255117
87.522265	3064.469431	22.260135
87.720373	3063.383767	22.265152
87.575001	3061.759217	22.270170
87.809146	3055.218212	22.275187
87.648620	3063.470573	22.280205
87.904754	3069.725030	22.285223
87.961260	3055.975083	22.290240
87.748593	3058.342596	22.295258
88.017838	3053.987041	22.300275
87.965125	3064.030176	22.305293
88.120791	3068.373751	22.310311
88.241064	3083.741646	22.315328
87.780186	3082.113327	22.320346
88.343173	3075.794340	22.325363
88.313611	3086.980469	22.330381
88.223735	3087.114788	22.335399
88.290003	3096.389886	22.340416
88.349808	3106.042421	22.345434
88.354666	3120.286946	22.350451
88.497805	3120.474884	22.355469
88.699038	3123.752322	22.360487
88.707860	3142.360229	22.365504
88.904602	3148.613902	22.370522
89.320475	3134.951346	22.375539
89.209986	3149.084255	22.380557
88.950389	3149.795421	22.385575
89.567034	3158.397738	22.390592
89.473693	3181.970046	22.395610
89.624698	3179.655584	22.400627
89.745743	3173.591471	22.405645
89.929440	3173.442797	22.410663
90.351583	3162.093279	22.415680
90.060467	3164.763132	22.420698
90.337627	3157.515392	22.425715
89.979423	3176.626889	22.430733
90.252977	3181.226598	22.435751
90.761336	3182.852955	22.440768
91.049497	3187.023494	22.445786
91.342372	3173.039902	22.450803
91.247063	3180.765817	22.455821
90.582901	3170.078857	22.460839
90.847516	3167.159028	22.465856
91.262444	3175.999406	22.470874
91.244352	3174.912455	22.475891
91.391384	3183.408536	22.480909
91.392625	3179.196836	22.485927
91.227028	3179.491302	22.490944
91.308209	3186.437293	22.495962
91.148460	3175.954762	22.500979
91.369666	3190.300998	22.505997
91.223376	3203.307624	22.511015
91.725974	3207.603752	22.516032
91.666411	3214.781669	22.521050
91.891645	3215.047771	22.526067
92.020456	3227.376693	22.531085
92.016981	3233.342629	22.536103
92.381310	3230.931887	22.541120
92.391588	3249.250714	22.546138
92.495164	3239.658065	22.551155
92.205885	3236.349058	22.556173
92.308620	3246.380008	22.561191
92.759249	3261.767503	22.566208
92.880284	3269.124651	22.571226
92.976210	3269.050320	22.576243
93.489847	3278.330339	22.581261
93.094765	3267.461842	22.586279
93.545824	3263.532472	22.591296
93.520997	3262.917087	22.596314
93.680812	3252.365557	22.601331
93.830943	3255.690443	22.606349
94.058380	3248.474499	22.611367
94.105699	3256.785135	22.616384
93.664232	3255.080756	22.621402
93.741350	3255.100870	22.626419
93.923107	3251.514815	22.631437
94.033383	3256.664741	22.636455
94.097298	3255.946506	22.641472
94.032636	3257.604965	22.646490
94.370786	3277.312520	22.651507
94.232715	3281.053530	22.656525
94.132377	3287.299266	22.661543
94.374391	3284.645742	22.666560
94.062868	3289.982306	22.671578
94.259742	3304.341723	22.676595
94.112754	3309.305838	22.681613
94.260687	3306.386761	22.686631
94.643173	3331.203864	22.691648
95.066675	3345.098715	22.696666
95.029474	3341.848027	22.701683
95.111972	3342.175513	22.706701
94.993815	3345.261294	22.711719
95.373245	3362.744468	22.716736
95.468143	3377.632211	22.721754
95.610811	3373.437639	22.726771
96.013392	3374.036243	22.731789
95.722644	3367.835775	22.736807
96.181436	3359.859911	22.741824
96.246837	3374.601741	22.746842
96.388777	3359.703178	22.751859
96.409118	3363.253468	22.756877
96.424154	3383.139745	22.761895
96.440893	3388.478397	22.766912
96.625801	3397.515570	22.771930
96.913074	3392.354989	22.776947
96.941427	3391.106807	22.781965
96.857872	3387.399605	22.786983
96.870269	3387.508366	22.792000
96.719079	3391.496448	22.797018
96.945901	3392.557945	22.802035
96.985926	3408.889012	22.807053
96.927177	3421.373489	22.812071
97.293977	3424.489383	22.817088
97.251917	3418.388743	22.822106
97.500694	3429.110234	22.827123
97.997703	3436.958080	22.832141
97.966165	3453.369915	22.837159
98.457811	3441.581157	22.842176
97.980176	3443.916136	22.847194
98.356440	3454.398471	22.852211
98.443423	3445.060008	22.857229
98.425436	3458.013756	22.862247
98.486770	3447.803559	22.867264
98.368721	3452.318455	22.872282
98.462135	3452.224461	22.877299
98.333048	3453.199109	22.882317
98.682230	3474.875536	22.887335
98.859867	3467.646854	22.892352
98.833903	3469.709565	22.897370
98.809515	3478.320354	22.902387
99.242622	3478.955649	22.907405
99.265237	3497.570365	22.912423
99.345660	3495.299409	22.917440
99.316516	3495.000079	22.922458
99.209623	3508.460681	22.927475
99.710638	3496.682931	22.932493
100.018015	3519.951350	22.937511
100.317131	3521.747360	22.942528
99.753638	3538.473563	22.947546
100.451466	3526.417602	22.952563
100.384693	3517.068283	22.957581
100.435727	3532.039800	22.962599
100.491513	3520.982448	22.967616
100.778180	3513.876278	22.972634
100.551798	3516.735098	22.977651
100.884868	3517.352674	22.982669
100.484003	3526.230029	22.987687
101.091736	3525.421524	22.992704
100.914478	3533.794615	22.997722
101.140414	3548.334101	23.002739
100.979694	3551.276957	23.007757
101.254239	3553.284115	23.012775
101.520691	3554.628444	23.017792
101.362041	3555.390662	23.022810
101.074334	3551.591172	23.027827
101.633062	3569.823687	23.032845
101.642796	3583.222168	23.037863
101.866635	3579.080663	23.042880
102.045217	3583.669021	23.047898
101.946193	3584.886344	23.052915
102.023705	3579.049345	23.057933
101.843162	3582.504534	23.062951
102.011268	3588.764299	23.067968
102.211807	3607.159982	23.072986
102.084372	3603.391870	23.078003
102.658975	3613.374218	23.083021
102.445429	3641.937933	23.088039
103.064584	3630.058278	23.093056
103.157735	3648.397740	23.098074
103.017062	3644.260546	23.103091
103.389474	3639.692506	23.108109
102.964579	3642.842418	23.113127
103.469138	3645.180477	23.118144
103.558674	3659.583552	23.123162
103.434854	3670.602607	23.128179
103.921107	3655.836628	23.133197
103.887082	3663.091633	23.138215
103.935757	3657.382598	23.143232
104.331130	3663.826492	23.148250
104.074333	3657.866753	23.153267
104.664950	3652.371315	23.158285
104.603533	3653.734792	23.163303
104.461778	3648.682423	23.168320
104.535373	3654.844447	23.173338
104.646828	3682.634060	23.178355
104.794045	3681.930387	23.183373
104.556125	3684.069883	23.188391
104.243167	3691.712332	23.193408
105.050467	3703.234635	23.198426
105.278265	3717.036569	23.203443
105.327847	3709.795865	23.208461
105.511554	3713.008215	23.213479
105.596625	3714.710090	23.218496
105.664785	3708.843091	23.223514
105.658542	3714.534865	23.228531
105.685377	3716.386522	23.233549
105.584675	3739.450655	23.238567
105.809379	3745.175932	23.243584
106.205185	3739.322103	23.248602
105.950679	3745.524206	23.253619
106.415590	3748.584190	23.258637
106.424985	3774.147516	23.263655
106.587435	3772.546828	23.268672
106.723604	3770.394181	23.273690
106.912504	3774.198209	23.278707
106.760055	3769.707413	23.283725
106.532047	3782.995351	23.288743
107.119858	3796.765819	23.293760
107.096355	3802.917174	23.298778
107.322524	3803.872115	23.303795
107.550888	3797.832546	23.308813
107.338920	3809.794619	23.313831
107.307950	3810.025510	23.318848
107.572142	3818.958095	23.323866
107.489968	3825.597899	23.328883
107.809593	3828.416944	23.333901
108.207697	3833.767140	23.338919
108.035074	3840.851822	23.343936
108.414783	3856.680374	23.348954
108.218494	3855.736995	23.353971
108.472271	3857.951171	23.358989
108.532037	3857.782026	23.364007
108.638535	3854.467328	23.369024
108.609193	3864.518928	23.374042
108.551971	3860.641118	23.379059
109.145962	3866.016438	23.384077
108.890455	3885.218921	23.389095
108.905749	3878.864524	23.394112
109.176330	3881.471602	23.399130
109.082399	3885.338535	23.404147
109.532311	3895.497973	23.409165
109.552253	3903.965449	23.414183
109.600439	3918.787414	23.419200
109.791220	3912.885509	23.424218
109.805438	3908.002954	23.429235
110.146948	3909.266013	23.434253
110.151944	3918.195422	23.439271
110.245300	3917.561270	23.444288
110.710434	3928.120975	23.449306
110.576915	3928.932996	23.454323
111.044423	3925.046415	23.459341
111.017599	3929.685354	23.464359
110.521129	3927.791557	23.469376
110.713843	3928.376439	23.474394
111.004864	3944.861478	23.479411
111.261798	3949.000770	23.484429
111.343529	3955.129284	23.489447
111.399066	3958.974293	23.494464
111.740382	3949.843505	23.499482
111.399090	3958.586061	23.504499
112.011116	3971.757791	23.509517
111.827580	3982.126292	23.514535
111.613920	3990.739505	23.519552
111.744208	3987.129503	23.524570
112.025178	3992.673524	23.529587
112.079137	3997.794419	23.534605
112.332447	4013.332594	23.539623
112.287840	4018.903651	23.544640
112.903979	4010.529008	23.549658
112.548763	4019.458942	23.554675
112.951444	4020.923718	23.559693
113.441208	4026.732074	23.564711
113.153509	4039.964345	23.569728
113.529938	4025.353571	23.574746
113.476079	4040.951980	23.579763
113.519898	4028.083211	23.584781
113.198381	4022.656085	23.589799
113.892155	4029.113423	23.594816
114.210132	4015.456039	23.599834
114.015070	4034.027443	23.604851
114.425465	4046.950660	23.609869
114.435972	4044.978586	23.614887
114.345743	4049.614651	23.619904
114.483516	4044.242728	23.624922
114.060526	4066.806652	23.629939
114.085808	4056.650439	23.634957
114.561012	4068.565303	23.639975
114.899835	4082.850016	23.644992
114.988741	4077.472770	23.650010
114.623908	4090.433964	23.655027
114.922245	4089.459626	23.660045
115.123885	4098.232232	23.665063
115.002538	4109.960656	23.670080
115.315666	4114.825766	23.675098
115.409288	4126.558446	23.680115
115.650151	4124.097891	23.685133
115.759612	4141.198196	23.690151
115.623792	4148.682853	23.695168
115.937456	4140.127801	23.700186
115.744744	4148.753389	23.705203
115.955109	4156.275730	23.710221
116.237423	4171.285238	23.715239
116.226093	4170.640814	23.720256
116.378826	4170.054322	23.725274
116.515129	4176.167607	23.730291
116.691799	4190.220150	23.735309
116.903269	4207.402888	23.740327
117.245684	4206.677567	23.745344
117.545610	4204.261179	23.750362
117.516589	4208.079276	23.755379
117.523569	4200.756798	23.760397
117.656792	4205.794189	23.765415
117.317558	4210.441526	23.770432
117.804997	4225.697122	23.775450
117.749430	4234.946181	23.780467
117.928895	4242.691788	23.785485
118.200236	4233.476725	23.790503
118.082424	4243.676265	23.795520
118.518774	4250.642393	23.800538
118.325500	4257.400743	23.805555
118.593113	4261.016681	23.810573
118.917503	4252.976350	23.815591
118.924263	4252.852181	23.820608
119.057075	4255.161210	23.825626
119.029218	4254.502190	23.830643
119.335816	4267.514792	23.835661
119.696371	4276.019105	23.840679
119.644417	4280.430401	23.845696
119.706633	4284.534240	23.850714
119.626891	4276.788637	23.855731
119.852418	4284.647525	23.860749
120.080865	4273.878443	23.865767
119.728970	4282.381583	23.870784
120.146973	4300.715775	23.875802
120.292752	4306.519265	23.880819
120.501819	4316.656964	23.885837
120.959990	4305.094358	23.890855
120.477786	4315.213994	23.895872
120.603632	4331.431844	23.900890
120.635065	4331.745348	23.905907
120.791007	4348.006670	23.910925
121.008190	4333.079782	23.915943
121.048531	4344.156048	23.920960
121.612606	4358.697507	23.925978
121.793915	4358.069671	23.930995
121.568463	4366.816935	23.936013
121.999607	4363.013033	23.941031
122.022109	4358.347875	23.946048
122.254275	4355.513114	23.951066
121.925599	4364.258929	23.956083
122.131580	4374.446785	23.961101
122.333042	4394.035821	23.966119
122.246366	4396.952819	23.971136
122.623370	4386.448101	23.976154
122.443036	4397.373460	23.981171
122.284458	4405.019881	23.986189
122.804987	4415.804242	23.991207
122.587745	4431.580047	23.996224
123.225045	4428.385794	24.001242
123.343066	4455.665444	24.006259
123.099047	4447.215369	24.011277
123.731886	4442.644225	24.016295
123.591836	4457.806090	24.021312
124.020865	4459.448061	24.026330
124.026523	4470.886859	24.031347
124.461226	4480.533027	24.036365
124.610475	4478.372216	24.041383
124.324706	4474.607612	24.046400
124.613454	4476.218826	24.051418
124.411671	4467.930274	24.056435
124.199085	4469.626297	24.061453
124.729337	4478.616092	24.066471
124.631549	4497.092441	24.071488
124.822679	4500.421058	24.076506
125.239494	4510.998597	24.081523
125.091349	4503.950835	24.086541
125.282646	4510.219740	24.091559
125.439776	4534.262577	24.096576
125.731142	4527.601654	24.101594
125.550851	4532.870494	24.106611
125.759618	4534.535090	24.111629
126.224219	4546.128041	24.116647
126.087556	4557.590025	24.121664
126.387026	4561.953569	24.126682
126.313263	4559.985905	24.131699
126.512407	4561.070565	24.136717
126.570197	4567.574558	24.141735
126.544505	4570.974847	24.146752
126.673540	4593.540444	24.151770
126.743151	4589.795440	24.156787
126.780618	4595.332667	24.161805
127.079711	4605.695063	24.166823
127.310602	4620.443014	24.171840
127.239615	4625.441053	24.176858
127.515112	4624.314543	24.181875
127.721308	4636.262484	24.186893
128.186720	4647.592761	24.191911
127.850203	4649.368734	24.196928
128.213366	4654.745858	24.201946
128.253993	4661.082243	24.206963
127.934307	4680.607351	24.211981
128.563553	4681.667015	24.216999
128.448116	4688.896578	24.222016
128.603445	4696.999966	24.227034
128.921075	4703.699284	24.232051
129.061981	4718.975223	24.237069
129.423303	4705.280939	24.242087
129.099606	4705.663370	24.247104
129.332189	4725.992612	24.252122
129.621329	4720.001311	24.257139
129.821354	4734.280817	24.262157
130.302847	4724.286990	24.267175
130.032465	4734.378980	24.272192
130.072292	4727.404395	24.277210
130.582679	4743.219345	24.282227
130.540379	4752.788981	24.287245
130.671195	4751.912763	24.292263
130.673124	4762.139708	24.297280
131.053106	4761.994024	24.302298
131.135766	4763.697201	24.307315
130.817308	4759.487898	24.312333
131.203424	4781.969946	24.317351
131.198601	4790.935339	24.322368
131.046966	4782.463123	24.327386
131.665302	4791.133800	24.332403
131.202525	4804.011760	24.337421
131.729198	4794.995533	24.342439
131.685947	4812.231659	24.347456
131.744892	4822.894137	24.352474
132.073540	4834.615288	24.357491
132.166510	4842.084520	24.362509
132.601109	4839.310325	24.367527
132.554674	4845.569432	24.372544
132.490562	4860.097045	24.377562
132.619602	4878.832056	24.382579
132.367386	4883.419932	24.387597
132.655411	4884.871060	24.392615
132.826372	4902.175047	24.397632
133.109349	4906.328798	24.402650
133.012283	4910.934356	24.407667
132.959220	4928.352561	24.412685
133.574768	4928.649879	24.417703
133.468424	4938.216037	24.422720
134.305325	4953.781563	24.427738
134.815852	4959.030892	24.432755
134.546754	4958.866860	24.437773
134.935753	4952.574695	24.442791
135.192929	4961.669348	24.447808
134.912237	4959.920094	24.452826
135.312025	4948.771813	24.457843
134.946327	4952.924094	24.462861
134.966078	4945.405439	24.467879
135.094635	4949.553220	24.472896
135.559307	4968.259653	24.477914
135.481703	4974.658618	24.482931
135.605589	4982.852397	24.487949
135.605306	4976.958434	24.492967
135.585942	4989.602633	24.497984
135.762336	5016.714549	24.503002
136.324951	5008.008037	24.508019
135.644794	5023.677055	24.513037
136.173224	5027.980454	24.518055
136.628362	5034.165419	24.523072
136.473803	5041.287819	24.528090
137.009723	5042.386556	24.533107
137.419937	5063.491287	24.538125
137.852571	5051.905185	24.543143
138.179256	5044.113305	24.548160
138.097085	5048.972370	24.553178
138.625593	5038.005924	24.558195
138.334295	5038.591687	24.563213
138.281584	5013.656695	24.568231
138.246638	5021.658611	24.573248
138.481134	5038.470714	24.578266
138.549865	5034.150896	24.583283
138.684428	5045.960581	24.588301
138.555146	5046.226240	24.593319
138.756192	5045.886480	24.598336
138.892621	5050.720449	24.603354
139.153358	5046.289366	24.608371
139.062803	5062.413802	24.613389
139.200307	5077.429608	24.618407
139.084802	5074.536804	24.623424
139.146497	5097.795815	24.628442
139.477548	5099.832822	24.633459
139.220522	5106.266213	24.638477
139.506720	5112.259813	24.643495
139.804455	5135.407823	24.648512
139.793154	5141.580527	24.653530
140.077318	5157.839618	24.658547
140.250094	5172.085441	24.663565
140.530852	5171.958907	24.668583
140.679734	5173.249574	24.673600
140.499629	5196.568373	24.678618
140.946842	5194.666133	24.683635
140.740935	5211.269276	24.688653
140.944729	5218.423496	24.693671
141.203202	5230.036450	24.698688
141.255385	5233.713414	24.703706
142.060710	5250.893280	24.708723
142.447978	5242.619984	24.713741
142.468845	5247.457753	24.718759
142.355251	5249.965143	24.723776
142.641474	5249.223865	24.728794
142.346265	5249.818550	24.733811
142.372791	5240.655162	24.738829
142.741362	5245.388621	24.743847
143.161252	5253.610411	24.748864
142.653114	5274.676998	24.753882
142.813546	5274.910933	24.758899
142.837413	5280.310085	24.763917
142.964585	5289.757548	24.768935
143.367335	5300.167852	24.773952
143.467828	5312.688166	24.778970
143.990183	5308.995358	24.783987
144.240688	5337.797732	24.789005
144.263383	5342.578923	24.794023
144.846745	5345.576347	24.799040
144.395045	5341.615697	24.804058
144.691042	5338.521762	24.809075
144.875648	5346.343850	24.814093
144.987078	5349.318457	24.819111
145.033060	5353.292962	24.824128
144.938614	5370.520839	24.829146
145.273537	5362.078946	24.834163
145.225899	5375.901090	24.839181
145.367814	5379.773914	24.844199
145.447494	5391.429919	24.849216
145.468857	5406.688879	24.854234
145.741080	5411.047322	24.859251
145.979285	5431.195431	24.864269
145.560298	5428.423187	24.869287
146.039450	5452.211450	24.874304
146.383655	5466.582383	24.879322
147.149133	5457.023112	24.884339
147.306169	5468.953434	24.889357
147.477280	5458.918686	24.894375
148.153431	5464.999187	24.899392
148.115574	5458.892327	24.904410
148.059968	5461.641772	24.909427
148.319511	5461.276589	24.914445
148.244867	5462.384111	24.919463
148.444026	5463.007364	24.924480
148.267116	5459.924611	24.929498
148.247358	5469.810681	24.934515
148.747752	5455.999053	24.939533
148.283566	5458.172630	24.944551
148.602783	5480.241889	24.949568
148.383665	5486.043115	24.954586
148.563263	5492.200556	24.959603
148.729588	5524.695170	24.964621
148.886989	5520.271579	24.969639
149.265891	5531.561674	24.974656
148.974717	5555.873491	24.979674
149.558952	5552.464927	24.984691
150.060962	5576.912280	24.989709
149.927391	5590.206227	24.994727
150.004140	5581.566690	24.999744
149.848395	5609.462164	25.004762
150.022194	5610.842068	25.009779
150.320115	5624.161214	25.014797
150.658703	5631.412264	25.019815
151.332632	5644.231447	25.024832
151.112279	5663.708682	25.029850
151.168500	5654.887827	25.034867
151.473758	5655.017512	25.039885
151.152169	5668.104374	25.044903
151.831332	5677.783344	25.049920
151.854380	5680.117023	25.054938
152.094109	5683.283514	25.059955
152.072021	5690.954865	25.064973
152.000763	5705.765188	25.069991
152.273668	5709.585343	25.075008
152.322816	5706.373050	25.080026
152.596738	5724.614602	25.085043
152.640879	5728.828908	25.090061
152.836922	5735.297549	25.095079
153.105922	5738.652548	25.100096
153.087973	5751.065207	25.105114
153.536566	5765.001001	25.110131
153.538050	5769.997666	25.115149
153.368608	5768.042510	25.120167
154.028463	5776.821856	25.125184
154.082855	5794.076398	25.130202
154.041606	5785.446008	25.135219
154.204291	5790.901937	25.140237
154.409047	5811.627794	25.145255
154.657719	5818.011385	25.150272
154.897041	5824.195314	25.155290
154.824879	5828.083148	25.160307
154.907277	5844.566870	25.165325
155.162001	5844.974630	25.170343
155.601283	5844.612816	25.175360
155.369496	5875.342583	25.180378
155.461208	5886.015334	25.185395
155.385727	5894.770562	25.190413
155.087515	5911.853936	25.195431
155.842457	5910.975722	25.200448
156.007919	5934.095189	25.205466
156.331860	5946.158161	25.210483
156.775410	5948.752761	25.215501
157.023971	5980.212141	25.220519
157.188099	5972.470684	25.225536
157.276032	5967.801323	25.230554
157.486289	5983.390315	25.235571
157.786524	5993.703045	25.240589
157.907846	6006.923726	25.245607
158.504340	6000.311779	25.250624
158.043225	6008.646073	25.255642
158.231061	6011.916496	25.260659
158.296615	6001.407433	25.265677
158.492768	6030.386621	25.270695
158.782529	6034.702572	25.275712
158.287695	6044.320601	25.280730
158.809583	6044.278649	25.285747
159.181008	6060.547493	25.290765
159.060527	6074.909141	25.295783
159.470538	6071.823001	25.300800
159.551112	6094.107782	25.305818
159.056609	6094.599971	25.310835
159.503539	6103.418230	25.315853
159.948054	6132.977926	25.320871
160.273474	6118.707940	25.325888
160.063863	6137.058220	25.330906
160.182945	6161.975731	25.335923
160.774638	6157.701891	25.340941
160.859112	6170.247588	25.345959
160.828968	6181.822312	25.350976
160.850958	6192.464660	25.355994
161.328897	6203.473479	25.361011
161.276233	6215.327584	25.366029
161.458664	6224.557391	25.371047
161.991106	6226.258862	25.376064
161.625359	6247.156739	25.381082
161.946021	6258.458559	25.386099
162.586034	6252.018086	25.391117
162.274547	6259.343374	25.396135
162.540088	6277.060095	25.401152
162.944346	6271.689450	25.406170
162.993477	6285.907497	25.411187
163.471406	6288.319673	25.416205
163.326572	6300.784447	25.421223
163.521504	6302.570833	25.426240
163.658015	6308.588841	25.431258
163.689367	6308.399559	25.436275
164.164047	6310.469698	25.441293
164.328675	6314.592982	25.446311
164.496637	6322.763642	25.451328
164.526705	6340.324035	25.456346
164.280128	6339.009611	25.461363
164.998664	6338.920203	25.466381
164.986517	6349.246196	25.471399
164.899013	6347.638512	25.476416
165.078063	6366.786403	25.481434
165.236321	6367.631450	25.486451
165.463531	6367.129441	25.491469
165.181632	6400.813509	25.496487
165.668043	6408.262975	25.501504
166.103975	6417.808552	25.506522
166.279734	6423.268054	25.511539
166.391723	6421.586447	25.516557
166.004130	6439.173435	25.521575
166.503345	6444.467668	25.526592
167.039889	6461.528687	25.531610
166.964570	6452.312117	25.536627
167.376937	6471.387720	25.541645
167.504884	6477.615120	25.546663
167.988338	6467.684841	25.551680
168.360439	6475.935257	25.556698
168.328442	6461.262519	25.561715
168.286150	6473.202522	25.566733
168.542888	6488.628403	25.571751
168.749275	6495.895005	25.576768
169.121543	6500.863714	25.581786
169.020444	6499.256686	25.586803
169.320165	6507.507265	25.591821
169.327531	6507.583408	25.596839
169.244905	6509.118776	25.601856
169.336057	6511.553157	25.606874
169.622148	6519.383083	25.611891
170.013308	6526.858583	25.616909
169.855357	6532.689857	25.621927
170.213909	6547.587856	25.626944
170.222314	6557.104930	25.631962
170.245834	6568.145778	25.636979
170.869175	6571.687729	25.641997
170.714290	6592.507120	25.647015
170.842988	6589.937530	25.652032
171.103406	6596.282484	25.657050
171.566601	6622.970192	25.662067
171.882930	6621.707641	25.667085
171.564016	6623.178894	25.672103
171.658471	6632.424266	25.677120
171.734392	6636.547328	25.682138
171.384434	6644.027997	25.687156
171.472406	6662.935345	25.692173
171.933676	6689.828248	25.697191
172.157730	6697.312540	25.702208
172.794522	6704.431730	25.707226
172.835550	6724.067520	25.712244
173.342094	6724.354153	25.717261
173.314746	6740.947913	25.722279
173.400891	6738.361704	25.727296
173.758437	6761.181306	25.732314
173.918590	6773.376331	25.737332
174.023467	6773.697044	25.742349
174.370135	6776.601159	25.747367
174.349676	6796.168443	25.752384
174.652448	6803.641354	25.757402
174.427004	6808.120617	25.762420
174.742306	6806.666845	25.767437
175.009666	6822.777263	25.772455
175.391844	6819.774336	25.777472
175.830278	6811.359458	25.782490
175.489239	6812.338221	25.787508
176.053892	6830.757477	25.792525
176.206032	6843.442168	25.797543
176.413745	6844.883916	25.802560
176.841481	6840.388906	25.807578
176.818926	6840.462119	25.812596
176.637933	6849.106544	25.817613
176.401198	6852.489826	25.822631
176.613388	6869.976614	25.827648
176.988957	6877.313097	25.832666
177.072154	6899.630877	25.837684
177.160609	6902.964374	25.842701
177.424352	6917.695676	25.847719
177.611288	6941.679398	25.852736
177.756430	6949.803752	25.857754
178.007164	6970.996870	25.862772
178.044901	6978.539647	25.867789
178.418032	6988.296780	25.872807
178.462712	7004.796221	25.877824
178.868660	7001.711364	25.882842
178.835744	7025.623644	25.887860
179.674886	7028.562994	25.892877
179.529475	7031.505936	25.897895
179.650369	7040.770806	25.902912
180.127663	7045.493941	25.907930
180.244166	7056.783604	25.912948
180.680268	7054.315147	25.917965
180.363051	7074.103500	25.922983
180.344777	7084.931096	25.928000
180.600219	7078.722377	25.933018
180.684110	7098.233414	25.938036
180.893722	7108.620922	25.943053
181.408500	7121.054536	25.948071
181.379462	7129.032921	25.953088
181.862813	7142.787784	25.958106
181.897394	7158.305372	25.963124
182.128081	7150.333395	25.968141
182.514140	7168.615591	25.973159
182.555311	7184.526693	25.978176
182.659832	7185.553931	25.983194
182.387968	7192.499002	25.988212
182.623889	7205.174079	25.993229
182.674919	7221.154471	25.998247
182.948163	7238.267719	26.003264
183.221389	7254.609946	26.008282
182.986996	7263.370532	26.013300
183.498479	7279.689170	26.018317
183.673277	7300.523540	26.023335
183.846339	7320.474554	26.028352
184.400819	7327.528872	26.033370
184.557585	7344.871767	26.038388
184.827834	7348.487205	26.043405
184.866342	7358.535347	26.048423
185.204743	7373.999797	26.053440
185.361337	7376.277008	26.058458
185.218182	7380.423862	26.063476
185.495169	7394.266598	26.068493
185.634102	7412.926999	26.073511
185.826911	7415.414819	26.078528
186.406396	7430.253524	26.083546
186.469164	7438.828853	26.088564
186.572925	7432.551335	26.093581
186.881383	7459.701569	26.098599
186.848198	7470.450770	26.103616
187.317540	7467.616830	26.108634
187.209169	7477.810606	26.113652
187.600449	7489.159138	26.118669
187.827991	7493.307779	26.123687
187.951735	7491.717053	26.128704
188.562536	7486.421348	26.133722
188.624375	7500.714789	26.138740
188.815949	7514.659167	26.143757
189.039093	7519.566207	26.148775
188.724624	7524.630599	26.153792
188.895873	7510.138316	26.158810
188.995854	7534.016018	26.163828
189.315824	7539.103176	26.168845
189.654224	7558.415211	26.173863
189.550556	7568.824858	26.178880
190.363093	7576.232811	26.183898
190.324406	7587.174387	26.188916
190.519889	7586.576773	26.193933
190.966119	7601.852722	26.198951
190.681131	7604.553411	26.203968
190.955892	7595.439786	26.208986
190.872920	7621.590929	26.214004
191.118693	7629.417046	26.219021
191.628336	7632.915023	26.224039
191.636364	7652.106913	26.229056
191.420215	7668.651721	26.234074
191.583090	7679.942831	26.239092
192.105253	7690.817013	26.244109
192.754240	7693.145229	26.249127
192.908935	7709.487824	26.254144
193.346693	7708.073597	26.259162
193.340317	7725.299735	26.264180
193.462081	7711.069053	26.269197
193.894345	7722.930014	26.274215
193.615481	7743.008217	26.279232
194.170647	7742.686687	26.284250
194.146522	7752.956507	26.289268
193.926441	7761.404686	26.294285
194.327449	7773.046382	26.299303
194.491823	7791.810142	26.304320
194.768905	7802.498852	26.309338
194.787897	7814.658937	26.314356
195.055401	7821.341101	26.319373
195.475043	7835.088982	26.324391
195.148459	7848.272589	26.329408
195.463386	7859.101580	26.334426
195.837612	7880.193605	26.339444
195.951648	7905.456531	26.344461
196.430251	7906.192025	26.349479
196.636233	7913.807477	26.354496
197.152039	7920.128097	26.359514
197.075478	7935.283608	26.364532
197.273062	7948.279088	26.369549
197.590058	7947.677136	26.374567
197.555249	7973.336519	26.379584
197.621464	7974.140942	26.384602
197.791784	7984.859231	26.389620
198.070716	7998.980994	26.394637
198.414390	8005.061512	26.399655
198.348342	8018.018697	26.404672
198.791207	8032.677339	26.409690
198.663386	8045.028047	26.414708
198.921772	8058.508984	26.419725
199.369538	8064.945659	26.424743
199.285677	8072.320021	26.429760
199.482954	8083.389927	26.434778
199.830948	8091.392352	26.439796
199.793912	8104.778794	26.444813
199.923182	8119.897321	26.449831
200.109404	8125.045363	26.454848
200.273030	8145.270709	26.459866
200.641258	8155.668930	26.464884
200.585102	8172.318573	26.469901
200.850008	8180.395418	26.474919
201.231244	8206.533049	26.479936
201.337382	8218.699523	26.484954
201.927087	8224.523664	26.489972
201.795352	8239.607456	26.494989
202.155972	8250.999411	26.500007
202.110277	8272.236168	26.505024
202.542135	8282.831106	26.510042
203.000741	8291.858969	26.515060
203.064269	8313.662945	26.520077
203.587111	8323.085056	26.525095
203.679066	8327.365014	26.530112
203.627379	8331.973522	26.535130
204.168632	8343.680682	26.540148
204.367199	8350.889575	26.545165
204.701413	8335.556772	26.550183
204.974762	8359.751272	26.555200
204.859981	8367.824787	26.560218
205.499603	8370.368106	26.565236
205.734931	8385.110201	26.570253
205.995521	8364.772285	26.575271
205.912107	8379.607997	26.580288
206.052766	8396.797968	26.585306
206.232944	8398.820175	26.590324
206.123300	8407.731697	26.595341
206.702745	8423.377888	26.600359
206.828506	8444.140742	26.605376
206.917235	8441.495543	26.610394
206.742127	8450.915694	26.615412
207.012216	8466.164087	26.620429
207.393530	8471.607666	26.625447
207.488144	8498.209012	26.630464
207.406045	8503.864646	26.635482
207.439654	8521.664748	26.640500
207.611103	8555.117814	26.645517
207.837856	8568.646947	26.650535
207.986122	8582.456859	26.655552
208.200198	8600.984161	26.660570
208.861926	8618.752265	26.665588
208.887960	8642.121645	26.670605
209.179102	8656.774430	26.675623
209.279807	8668.879136	26.680640
209.612662	8688.991360	26.685658
209.867790	8700.728734	26.690676
210.224466	8727.225727	26.695693
210.636707	8730.370637	26.700711
210.529332	8747.337318	26.705728
211.092881	8759.467225	26.710746
211.440433	8762.906386	26.715764
211.268734	8790.787269	26.720781
211.794117	8790.331231	26.725799
211.691981	8809.577382	26.730816
211.925046	8824.729054	26.735834
212.196552	8823.952640	26.740852
212.537438	8855.699055	26.745869
213.145042	8843.405072	26.750887
213.405691	8858.441947	26.755904
213.241434	8851.411827	26.760922
213.488680	8876.217927	26.765940
213.502291	8892.702415	26.770957
213.980325	8894.855848	26.775975
213.737856	8904.451230	26.780992
213.953731	8922.978611	26.786010
213.848956	8928.657834	26.791028
214.178557	8956.110393	26.796045
214.479278	8953.868026	26.801063
214.612649	8978.120467	26.806080
214.797008	8988.353488	26.811098
215.029687	9001.700848	26.816116
215.185237	9021.731730	26.821133
215.432345	9031.102153	26.826151
215.539309	9052.892091	26.831168
215.709809	9081.249407	26.836186
216.365312	9086.460431	26.841204
216.631641	9104.556707	26.846221
216.977833	9114.705571	26.851239
216.924887	9120.255784	26.856256
217.123658	9138.996552	26.861274
217.535541	9140.474096	26.866292
217.484413	9166.584715	26.871309
218.048292	9180.328053	26.876327
218.005704	9189.187184	26.881344
218.190937	9211.194409	26.886362
218.893486	9220.510173	26.891380
218.757806	9231.331064	26.896397
219.154790	9232.555872	26.901415
219.574055	9252.876660	26.906432
219.508343	9264.356329	26.911450
220.060923	9272.713090	26.916468
220.080769	9289.653027	26.921485
220.510613	9308.002146	26.926503
220.602682	9309.888581	26.931520
220.661078	9329.579871	26.936538
221.139847	9332.727301	26.941556
221.329359	9337.398646	26.946573
221.656287	9365.730624	26.951591
221.823093	9364.724938	26.956608
221.441643	9369.462274	26.961626
222.141926	9388.299277	26.966644
222.468623	9394.787222	26.971661
222.381588	9398.011610	26.976679
222.520653	9409.017231	26.981696
222.711697	9420.312018	26.986714
223.074292	9450.339661	26.991732
223.277758	9466.768169	26.996749
223.448803	9479.941008	27.001767
223.767962	9485.398359	27.006784
223.713144	9499.691608	27.011802
224.160070	9519.960120	27.016820
224.289127	9537.826721	27.021837
224.564040	9553.956793	27.026855
224.995261	9562.092725	27.031872
224.610558	9599.532671	27.036890
225.431166	9598.008557	27.041908
225.706339	9609.593629	27.046925
225.523036	9623.737288	27.051943
225.851106	9635.819342	27.056960
226.042355	9651.760898	27.061978
226.840522	9658.217527	27.066996
227.077004	9664.073786	27.072013
227.273825	9678.282295	27.077031
227.629044	9669.517324	27.082048
227.365644	9686.683290	27.087066
227.588481	9691.016035	27.092084
227.888080	9703.606187	27.097101
228.241235	9723.680923	27.102119
228.649009	9745.159802	27.107136
228.254416	9741.681297	27.112154
228.755080	9771.572517	27.117172
228.872588	9784.107746	27.122189
229.334970	9789.124054	27.127207
229.149709	9803.193363	27.132224
229.311902	9809.027291	27.137242
229.779190	9824.816284	27.142260
230.159592	9834.755153	27.147277
230.205862	9839.767760	27.152295
230.380684	9859.527116	27.157312
230.277857	9879.166163	27.162330
230.932731	9897.395286	27.167348
230.869618	9911.955733	27.172365
231.087281	9927.969610	27.177383
232.020402	9928.172452	27.182400
232.084522	9942.392093	27.187418
232.638237	9947.175953	27.192436
232.580973	9967.887538	27.197453
232.814873	9968.883344	27.202471
233.181472	9988.088917	27.207488
233.090734	10002.663465	27.212506
233.432048	10007.480073	27.217524
233.434304	10018.336210	27.222541
233.482944	10025.668314	27.227559
234.050523	10041.715079	27.232576
234.194086	10059.334099	27.237594
234.249365	10070.981047	27.242612
234.731258	10094.048800	27.247629
234.751244	10100.719260	27.252647
235.190829	10112.192461	27.257664
235.012016	10140.916590	27.262682
235.660051	10142.706541	27.267700
236.251632	10173.021468	27.272717
236.165279	10177.597638	27.277735
236.750590	10183.398817	27.282752
236.790949	10207.751998	27.287770
237.227859	10212.746655	27.292788
236.990333	10222.468834	27.297805
237.174631	10249.600245	27.302823
237.820112	10239.940196	27.307840
237.850507	10268.370826	27.312858
238.073177	10278.729112	27.317876
238.271210	10293.037223	27.322893
238.309956	10315.202514	27.327911
238.479936	10329.534986	27.332928
239.019389	10344.941551	27.337946
238.850772	10359.649814	27.342964
238.960601	10376.963604	27.347981
239.463035	10394.162917	27.352999
240.411193	10419.085634	27.358016
240.345256	10440.955664	27.363034
240.398996	10442.640605	27.368052
240.738867	10457.012867	27.373069
240.357851	10475.239715	27.378087
241.043424	10487.420897	27.383104
241.123571	10517.768990	27.388122
241.404157	10532.374046	27.393140
241.586746	10555.076778	27.398157
241.676144	10581.628897	27.403175
242.419261	10579.777196	27.408192
242.149469	10628.953736	27.413210
242.503522	10630.945140	27.418228
242.733475	10630.437830	27.423245
242.838908	10663.680147	27.428263
243.321085	10668.628083	27.433280
243.519430	10705.471697	27.438298
243.729466	10710.548112	27.443316
243.901587	10734.901593	27.448333
244.346908	10758.963406	27.453351
244.627751	10776.859883	27.458368
244.942157	10791.498188	27.463386
244.874952	10804.587020	27.468404
245.212757	10808.847508	27.473421
245.401060	10833.919264	27.478439
246.256054	10836.347062	27.483456
246.121745	10860.392145	27.488474
246.186638	10868.498682	27.493492
247.070626	10884.659449	27.498509
247.007445	10891.490504	27.503527
247.599170	10889.069811	27.508544
247.933413	10915.185787	27.513562
248.137769	10924.724307	27.518580
248.101613	10924.465773	27.523597
248.311344	10938.159650	27.528615
248.428614	10948.042644	27.533632
248.671294	10964.518209	27.538650
248.979287	10982.176464	27.543668
249.103582	11001.062495	27.548685
249.160487	11015.204718	27.553703
249.694800	11025.196104	27.558720
249.881687	11051.943230	27.563738
250.016401	11064.465592	27.568756
250.383836	11091.407468	27.573773
250.286529	11114.325820	27.578791
250.767742	11135.461999	27.583808
250.860955	11150.813877	27.588826
251.059818	11166.283811	27.593844
251.296996	11191.422102	27.598861
251.597263	11204.183489	27.603879
252.407204	11214.071159	27.608896
252.224692	11234.638854	27.613914
252.802381	11247.603377	27.618932
253.604831	11255.273926	27.623949
253.710523	11285.420732	27.628967
254.309777	11278.656494	27.633984
254.073199	11294.092933	27.639002
254.571923	11300.052208	27.644020
254.579140	11316.651331	27.649037
254.193138	11335.997839	27.654055
254.706024	11343.821048	27.659072
254.678634	11360.466899	27.664090
254.841257	11391.402522	27.669108
255.534508	11405.617992	27.674125
255.421305	11427.223025	27.679143
255.855614	11445.497454	27.684160
255.725048	11467.853022	27.689178
256.121075	11491.582968	27.694196
256.648012	11512.146456	27.699213
256.937107	11537.697394	27.704231
256.944005	11548.551436	27.709248
257.484958	11573.277751	27.714266
257.936533	11586.324048	27.719284
258.159147	11595.690575	27.724301
258.071650	11620.350631	27.729319
258.363326	11639.758853	27.734336
258.600218	11660.555586	27.739354
259.141359	11679.254586	27.744372
259.716439	11688.863085	27.749389
259.268831	11708.733864	27.754407
259.781932	11719.450817	27.759424
260.214705	11746.937612	27.764442
260.139397	11767.503243	27.769460
260.720264	11771.701774	27.774477
260.763293	11799.049011	27.779495
261.017338	11818.300590	27.784512
261.320012	11832.234336	27.789530
261.206133	11857.731827	27.794548
262.205900	11861.035549	27.799565
261.864782	11883.587194	27.804583
262.661547	11883.486458	27.809600
262.542403	11911.369604	27.814618
262.634411	11919.453284	27.819636
263.003683	11944.614260	27.824653
263.262003	11968.414145	27.829671
263.547146	11983.359321	27.834688
263.717807	12009.639610	27.839706
263.521294	12033.993730	27.844724
264.179296	12053.754745	27.849741
264.380712	12085.348637	27.854759
264.434721	12105.165388	27.859776
264.476124	12128.429390	27.864794
264.869133	12156.127500	27.869812
265.058477	12176.144145	27.874829
265.482635	12209.518989	27.879847
265.775049	12230.865066	27.884864
266.591925	12258.943172	27.889882
266.780379	12275.040642	27.894900
267.423248	12289.797009	27.899917
267.396924	12308.499110	27.904935
267.766770	12327.695927	27.909952
268.193345	12349.752680	27.914970
268.076133	12362.085266	27.919988
268.631284	12382.607393	27.925005
268.641795	12399.648275	27.930023
268.900468	12417.975677	27.935040
269.491426	12436.642119	27.940058
269.748830	12461.047942	27.945076
270.115591	12477.900055	27.950093
269.744945	12488.302648	27.955111
270.459799	12516.365759	27.960128
270.646581	12540.593501	27.965146
270.941026	12555.042907	27.970164
271.387062	12580.372611	27.975181
271.396773	12600.702297	27.980199
271.746847	12617.603795	27.985216
272.269463	12632.491432	27.990234
272.145049	12653.175815	27.995252
272.576072	12667.073323	28.000269
272.811813	12689.806531	28.005287
273.014271	12715.526495	28.010304
273.925801	12724.040857	28.015322
274.023403	12750.815013	28.020340
273.833641	12760.929481	28.025357
273.901880	12779.478630	28.030375
274.618645	12789.657637	28.035392
275.151663	12821.706351	28.040410
275.174202	12828.190012	28.045428
275.607309	12834.949349	28.050445
275.620667	12867.325094	28.055463
276.275391	12882.703244	28.060480
276.651290	12888.446262	28.065498
276.901206	12910.636968	28.070516
276.624648	12930.373048	28.075533
276.778407	12946.342985	28.080551
277.116058	12969.464710	28.085568
277.454182	12983.406203	28.090586
277.570259	13019.250790	28.095604
278.048500	13035.428776	28.100621
278.121025	13067.295639	28.105639
278.671689	13087.159962	28.110656
278.583493	13103.920080	28.115674
278.750026	13125.458320	28.120692
279.251102	13144.902305	28.125709
279.418264	13172.357418	28.130727
279.937479	13205.055230	28.135744
280.038229	13216.042220	28.140762
280.437893	13244.738552	28.145780
280.894321	13253.243297	28.150797
281.041134	13272.394573	28.155815
281.541063	13283.044629	28.160832
282.017977	13301.569402	28.165850
281.998788	13310.737364	28.170868
282.530426	13314.401592	28.175885
282.606784	13338.068107	28.180903
283.260772	13359.234607	28.185920
283.315670	13370.528673	28.190938
283.204662	13386.703516	28.195956
283.257344	13393.845821	28.200973
283.631644	13426.158324	28.205991
283.691792	13462.405499	28.211008
284.118762	13484.247858	28.216026
284.219790	13502.645872	28.221044
284.277949	13538.871485	28.226061
284.566198	13572.331482	28.231079
284.844104	13605.010091	28.236096
285.620982	13633.450969	28.241114
285.804278	13662.989019	28.246132
286.417944	13688.559076	28.251149
286.392089	13710.062120	28.256167
286.751822	13731.709492	28.261184
287.351675	13758.084024	28.266202
287.308543	13780.363734	28.271220
287.800778	13810.367874	28.276237
287.901774	13832.652209	28.281255
288.543148	13859.067319	28.286272
288.730483	13874.663885	28.291290
288.901132	13894.933938	28.296308
289.411309	13921.563075	28.301325
289.549684	13945.844254	28.306343
289.828480	13962.171156	28.311360
289.954308	13979.902193	28.316378
290.093632	14019.520824	28.321396
290.750172	14035.909882	28.326413
290.991760	14058.451796	28.331431
291.219742	14091.864517	28.336448
291.750545	14104.987228	28.341466
291.793945	14147.444341	28.346484
291.918585	14157.553432	28.351501
292.131143	14182.227700	28.356519
292.542650	14218.585552	28.361536
293.456140	14245.224229	28.366554
292.953064	14264.491927	28.371572
293.383643	14288.890807	28.376589
294.178711	14313.798389	28.381607
294.354590	14346.761668	28.386624
295.013790	14349.721138	28.391642
294.747693	14374.490536	28.396660
295.241523	14404.350534	28.401677
295.822191	14418.144459	28.406695
296.032640	14446.820601	28.411712
296.878784	14453.789734	28.416730
296.920982	14471.711621	28.421748
297.310982	14481.564330	28.426765
297.691763	14498.836205	28.431783
297.664112	14528.491050	28.436800
297.929934	14526.792643	28.441818
298.153216	14560.153523	28.446836
298.708302	14564.316873	28.451853
298.585589	14585.911143	28.456871
298.844402	14611.769788	28.461888
299.501410	14610.726923	28.466906
299.519468	14650.687032	28.471924
299.889439	14663.256841	28.476941
300.177930	14679.300779	28.481959
300.188938	14705.659098	28.486976
300.483816	14716.979064	28.491994
300.749994	14741.107941	28.497012
301.018272	14760.459956	28.502029
301.426845	14781.968287	28.507047
301.350677	14808.445184	28.512064
301.846124	14829.814729	28.517082
302.095728	14858.770367	28.522100
302.350418	14875.707320	28.527117
302.339192	14897.250489	28.532135
302.825835	14929.886246	28.537152
303.072084	14954.820873	28.542170
303.294047	15001.534058	28.547188
303.369592	15022.297158	28.552205
303.824268	15042.819567	28.557223
303.602408	15084.741431	28.562240
304.253984	15108.573942	28.567258
304.680037	15145.949517	28.572276
304.930733	15183.642546	28.577293
305.321100	15219.169303	28.582311
305.814231	15255.249653	28.587328
306.365760	15273.789571	28.592346
306.582119	15310.149009	28.597364
306.484545	15338.381184	28.602381
307.392074	15360.591095	28.607399
307.439713	15401.429114	28.612416
308.016941	15415.869026	28.617434
308.054717	15448.644594	28.622452
308.878051	15485.315470	28.627469
309.297453	15507.543188	28.632487
309.372695	15541.229967	28.637504
309.577055	15558.869374	28.642522
310.044403	15580.830810	28.647540
310.275309	15601.069393	28.652557
310.541564	15618.079278	28.657575
311.054043	15641.804744	28.662592
311.479912	15665.106430	28.667610
311.454389	15681.471152	28.672628
311.983043	15714.566455	28.677645
312.410755	15732.202245	28.682663
312.512362	15754.865769	28.687680
313.505455	15782.174651	28.692698
313.959280	15806.108623	28.697716
313.945467	15813.516712	28.702733
314.455320	15836.284687	28.707751
314.355141	15853.919565	28.712768
314.799552	15859.526246	28.717786
314.846943	15897.549224	28.722804
314.792157	15905.523607	28.727821
315.172904	15930.579345	28.732839
315.411193	15977.350935	28.737856
315.993853	15993.350719	28.742874
315.945962	16034.816020	28.747892
316.208279	16059.883642	28.752909
316.567815	16086.564853	28.757927
317.070217	16130.700681	28.762944
317.320533	16152.224358	28.767962
317.731524	16184.991750	28.772980
317.927611	16203.998067	28.777997
318.147526	16238.989405	28.783015
318.132345	16268.282854	28.788032
319.024437	16286.657338	28.793050
319.475553	16319.194571	28.798068
319.475866	16349.777967	28.803085
320.181380	16374.273242	28.808103
320.286923	16409.994640	28.813120
320.585751	16423.534230	28.818138
321.101960	16455.238277	28.823156
321.496757	16461.586233	28.828173
321.947867	16479.761130	28.833191
322.144968	16491.487772	28.838208
322.995438	16513.517981	28.843226
323.259079	16527.968134	28.848244
323.250853	16554.714018	28.853261
323.872071	16559.629782	28.858279
323.521743	16589.719929	28.863296
324.026061	16607.818407	28.868314
324.149464	16632.463825	28.873332
324.254385	16655.709621	28.878349
324.827224	16677.529018	28.883367
324.945575	16706.314179	28.888384
325.609950	16725.424985	28.893402
326.011453	16747.674684	28.898420
326.475470	16767.564132	28.903437
326.567857	16800.856644	28.908455
326.583173	16825.168739	28.913472
326.635926	16849.323380	28.918490
326.746132	16884.539112	28.923508
327.388950	16921.624452	28.928525
327.775187	16951.829989	28.933543
328.295116	16987.202059	28.938560
328.681972	17021.426711	28.943578
328.747777	17046.101179	28.948596
328.898573	17080.700667	28.953613
329.299393	17113.265123	28.958631
329.433237	17150.698280	28.963648
329.796444	17196.951497	28.968666
329.926362	17208.056145	28.973684
330.461584	17259.258553	28.978701
331.238250	17302.256806	28.983719
331.582814	17326.266215	28.988736
331.474217	17354.883528	28.993754
331.898089	17387.845061	28.998772
332.411496	17429.924112	29.003789
332.712355	17463.910131	29.008807
332.997174	17501.267129	29.013824
333.626398	17526.069897	29.018842
333.893407	17561.491291	29.023860
334.078703	17601.352152	29.028877
334.727944	17618.204694	29.033895
335.171044	17651.128901	29.038912
335.794199	17668.040971	29.043930
336.119728	17709.242319	29.048948
336.215672	17733.000226	29.053965
336.949995	17757.581077	29.058983
337.190001	17777.675833	29.064000
337.344703	17806.529415	29.069018
337.632018	17842.354716	29.074036
337.788573	17868.881637	29.079053
338.141657	17886.237327	29.084071
338.342722	17911.642591	29.089088
338.417852	17946.005779	29.094106
338.923003	17975.697045	29.099124
339.255378	18018.680726	29.104141
339.703404	18044.321231	29.109159
339.877180	18073.044455	29.114176
340.204054	18105.348827	29.119194
340.499579	18143.923930	29.124212
340.800149	18165.747727	29.129229
341.067205	18206.710934	29.134247
341.908161	18249.540265	29.139264
341.961481	18282.753952	29.144282
342.262399	18312.523700	29.149300
342.564351	18346.640608	29.154317
343.039729	18374.160718	29.159335
343.250877	18405.553234	29.164352
343.357289	18432.954705	29.169370
344.160165	18473.412345	29.174388
344.297467	18497.957375	29.179405
344.307132	18525.403354	29.184423
344.968036	18566.037573	29.189440
345.084956	18591.900713	29.194458
345.520434	18620.438212	29.199476
345.832155	18654.147463	29.204493
346.108529	18696.986108	29.209511
346.692514	18723.929280	29.214528
347.098766	18759.040202	29.219546
347.333747	18789.170059	29.224564
347.452733	18825.649507	29.229581
348.045716	18864.697324	29.234599
348.347376	18909.663489	29.239616
348.633911	18923.689515	29.244634
349.419521	18963.019424	29.249652
349.633541	18996.627290	29.254669
350.164923	19025.143338	29.259687
350.745324	19047.792192	29.264704
350.868765	19078.804820	29.269722
351.173660	19102.416678	29.274740
351.514871	19125.341601	29.279757
352.131422	19141.007833	29.284775
353.043825	19173.640012	29.289792
353.096949	19197.887873	29.294810
353.828563	19221.416795	29.299828
354.329386	19240.001104	29.304845
354.110274	19249.859586	29.309863
354.240610	19284.014659	29.314880
354.093630	19314.993586	29.319898
354.526765	19333.693220	29.324916
354.824275	19384.326713	29.329933
355.004360	19411.507976	29.334951
355.441419	19457.987041	29.339968
355.461498	19495.707548	29.344986
356.030652	19529.831616	29.350004
356.291182	19573.051889	29.355021
356.659633	19609.539137	29.360039
357.260299	19649.143989	29.365056
357.250008	19689.568692	29.370074
357.573228	19727.146637	29.375092
358.050696	19764.514749	29.380109
358.394263	19805.787693	29.385127
358.546407	19856.131360	29.390144
358.729389	19893.154313	29.395162
359.525942	19936.597526	29.400180
360.202192	19982.524637	29.405197
360.765147	20020.314287	29.410215
361.219524	20053.525162	29.415232
361.504234	20084.576079	29.420250
361.755122	20110.135697	29.425268
362.229114	20148.793173	29.430285
362.479112	20189.767244	29.435303
362.936059	20216.695996	29.440320
362.732371	20260.704132	29.445338
363.507048	20285.540612	29.450356
363.800859	20325.503594	29.455373
364.442368	20370.554715	29.460391
364.884253	20403.210293	29.465408
365.404957	20433.598603	29.470426
365.576055	20448.204626	29.475444
365.496833	20501.170674	29.480461
366.093606	20519.715342	29.485479
366.816100	20556.672711	29.490496
366.785193	20598.926978	29.495514
367.493730	20625.070740	29.500532
368.117039	20656.162948	29.505549
368.160771	20683.304176	29.510567
368.147834	20703.125817	29.515584
368.632099	20739.673655	29.520602
369.435054	20757.030550	29.525620
369.539602	20797.673859	29.530637
369.963738	20810.414415	29.535655
370.634514	20852.075730	29.540672
370.611232	20883.735512	29.545690
370.916565	20898.909358	29.550708
371.373167	20926.236588	29.555725
371.622474	20959.811056	29.560743
372.119307	20991.397730	29.565760
372.283122	21032.392835	29.570778
372.822774	21052.970181	29.575796
373.018298	21095.790519	29.580813
373.508800	21132.502142	29.585831
374.016880	21155.367612	29.590848
374.477167	21197.584810	29.595866
374.735691	21220.237777	29.600884
375.047425	21253.376862	29.605901
375.340355	21291.511962	29.610919
375.509663	21316.358551	29.615936
376.194015	21364.818452	29.620954
376.444202	21389.397966	29.625972
376.893036	21435.073412	29.630989
377.400878	21474.939146	29.636007
377.909571	21489.863948	29.641024
378.191261	21530.011537	29.646042
378.565811	21559.415477	29.651060
378.985712	21587.717851	29.656077
379.326401	21631.664881	29.661095
380.117648	21656.611029	29.666112
380.188076	21692.061086	29.671130
380.721139	21710.992827	29.676148
381.208220	21754.841898	29.681165
381.181860	21779.016772	29.686183
381.350911	21814.012508	29.691200
381.590459	21860.160396	29.696218
382.261111	21882.903833	29.701236
382.589487	21925.855694	29.706253
383.000085	21961.557557	29.711271
383.377989	21992.449999	29.716288
383.922290	22040.086785	29.721306
383.962243	22064.489180	29.726324
384.679528	22112.978912	29.731341
385.141857	22150.870411	29.736359
385.719053	22176.648880	29.741376
386.176956	22209.262770	29.746394
386.260703	22232.371661	29.751412
386.594689	22267.317445	29.756429
387.006629	22301.320220	29.761447
387.477936	22334.731484	29.766464
387.698679	22370.222780	29.771482
388.231234	22414.739279	29.776500
388.677125	22435.352735	29.781517
388.939595	22481.635708	29.786535
389.645964	22503.858530	29.791552
389.992646	22539.080269	29.796570
390.448975	22561.309786	29.801588
390.951290	22592.993173	29.806605
391.464499	22622.718201	29.811623
391.716770	22646.575532	29.816640
392.116262	22684.434468	29.821658
392.556558	22700.432736	29.826676
392.949208	22724.683224	29.831693
393.041654	22770.424328	29.836711
393.162073	22794.084494	29.841728
393.588652	22822.878189	29.846746
393.741213	22858.102707	29.851764
394.399274	22882.735277	29.856781
394.338740	22917.925750	29.861799
395.060173	22945.653991	29.866816
395.183630	22993.646802	29.871834
395.806252	23031.061296	29.876852
396.072354	23064.826399	29.881869
396.379053	23109.815636	29.886887
396.759283	23141.868672	29.891904
397.114456	23181.673804	29.896922
397.647235	23230.056911	29.901940
398.323906	23254.652264	29.906957
398.441013	23294.686195	29.911975
398.632152	23322.942563	29.916992
398.718631	23365.261646	29.922010
399.201525	23408.984851	29.927028
400.009959	23442.568091	29.932045
400.382706	23490.927926	29.937063
400.566099	23536.520481	29.942080
401.068866	23575.239441	29.947098
401.230416	23627.710417	29.952116
402.038270	23666.825405	29.957133
402.030699	23705.532788	29.962151
402.686541	23761.555350	29.967168
402.943973	23801.600410	29.972186
403.213523	23851.263379	29.977204
403.842784	23891.775442	29.982221
403.819481	23951.761285	29.987239
404.408963	23987.642869	29.992256
404.940819	24037.622556	29.997274
405.072631	24087.198595	30.002292
405.678173	24131.846322	30.007309
406.139152	24196.497582	30.012327
406.347243	24244.006916	30.017344
406.966651	24288.756835	30.022362
407.307138	24336.782247	30.027380
408.222744	24388.538131	30.032397
408.520767	24432.322900	30.037415
408.991894	24470.741655	30.042432
409.390400	24520.074645	30.047450
409.765560	24546.747907	30.052468
410.231384	24589.209210	30.057485
410.442373	24635.534962	30.062503
410.831946	24673.787890	30.067520
411.713952	24724.525405	30.072538
412.277655	24763.219668	30.077556
412.432241	24805.639894	30.082573
412.688160	24846.085033	30.087591
413.110551	24894.095337	30.092608
413.766484	24943.497409	30.097626
413.983481	24969.215077	30.102644
414.465476	25015.812468	30.107661
414.724379	25061.174304	30.112679
415.416570	25098.816830	30.117696
415.765654	25143.758731	30.122714
416.080061	25179.369746	30.127732
416.868555	25217.234736	30.132749
417.129103	25266.826060	30.137767
417.664758	25293.688439	30.142784
417.834289	25342.571224	30.147802
418.409510	25368.643466	30.152820
418.885618	25420.184946	30.157837
419.354016	25462.785196	30.162855
419.788767	25486.660534	30.167872
420.226565	25526.544247	30.172890
420.466228	25568.457165	30.177908
421.327411	25595.348245	30.182925
421.419938	25642.117340	30.187943
421.770770	25664.445633	30.192960
422.187041	25702.422077	30.197978
422.305083	25737.872733	30.202996
422.466919	25768.205371	30.208013
422.939655	25815.281136	30.213031
423.362588	25853.559588	30.218048
424.077569	25899.898559	30.223066
423.706531	25944.430096	30.228084
424.520770	25993.071046	30.233101
424.435929	26041.895350	30.238119
425.034238	26087.222768	30.243136
425.532569	26130.866847	30.248154
426.019557	26190.099746	30.253172
426.809075	26233.203967	30.258189
427.436547	26287.761904	30.263207
427.602983	26331.918648	30.268224
427.729442	26385.323299	30.273242
428.241874	26436.554331	30.278260
428.712030	26458.627401	30.283277
428.930944	26531.997861	30.288295
429.655067	26570.439482	30.293312
430.104054	26612.121674	30.298330
430.874458	26668.388776	30.303348
431.295135	26706.120705	30.308365
431.765682	26771.265865	30.313383
432.396149	26802.929633	30.318400
432.884979	26846.772658	30.323418
433.258811	26886.417783	30.328436
433.740866	26913.507620	30.333453
434.241287	26964.420497	30.338471
434.356557	26998.330288	30.343488
434.645798	27035.674620	30.348506
435.207598	27097.683377	30.353524
435.633777	27132.374761	30.358541
435.968049	27189.756482	30.363559
436.663131	27225.558049	30.368576
437.070270	27272.314314	30.373594
437.303149	27325.505597	30.378612
437.774993	27361.211849	30.383629
438.144027	27415.658357	30.388647
438.536351	27462.641534	30.393664
438.942233	27509.710917	30.398682
439.159485	27562.441846	30.403700
439.773405	27611.864876	30.408717
440.177811	27658.777200	30.413735
440.944012	27699.261492	30.418752
441.232590	27754.898892	30.423770
441.900428	27802.272769	30.428788
442.314362	27848.509025	30.433805
443.016216	27891.042050	30.438823
443.190836	27946.812447	30.443840
443.893935	27974.832652	30.448858
443.987248	28022.995984	30.453876
444.708579	28076.645127	30.458893
444.820035	28117.307954	30.463911
445.640402	28159.068184	30.468928
446.042072	28212.707468	30.473946
446.408924	28259.618167	30.478964
447.142623	28293.106606	30.483981
447.320239	28342.906623	30.488999
447.583966	28390.481354	30.494016
448.028293	28423.311270	30.499034
448.478692	28469.331825	30.504052
449.151613	28517.366091	30.509069
449.411398	28565.642227	30.514087
449.909630	28605.236061	30.519104
450.476278	28646.553606	30.524122
450.821437	28690.049683	30.529140
451.375499	28731.732268	30.534157
451.636513	28772.394010	30.539175
452.036969	28825.019670	30.544192
452.600500	28850.282141	30.549210
452.618018	28904.715706	30.554228
453.270985	28949.748278	30.559245
453.639859	28991.544095	30.564263
454.127991	29032.389744	30.569280
454.558097	29079.118720	30.574298
454.797441	29132.314497	30.579316
455.389123	29188.660364	30.584333
455.893197	29229.667879	30.589351
456.285249	29284.327825	30.594368
456.847921	29334.903035	30.599386
456.815735	29392.365223	30.604404
457.580921	29437.068225	30.609421
457.829892	29491.676750	30.614439
458.167031	29555.665187	30.619456
458.753238	29598.098489	30.624474
459.096080	29661.285110	30.629492
459.831358	29704.943265	30.634509
460.337937	29769.043301	30.639527
461.204891	29823.339427	30.644544
461.484504	29875.988234	30.649562
461.859158	29929.845500	30.654580
462.343150	29976.044319	30.659597
462.954454	30030.209815	30.664615
463.529619	30082.684241	30.669632
463.662564	30129.512449	30.674650
463.789353	30183.909883	30.679668
464.451731	30236.824641	30.684685
465.090904	30291.957993	30.689703
465.295164	30359.637100	30.694720
466.348276	30402.351721	30.699738
466.450619	30466.764012	30.704756
467.304339	30517.972853	30.709773
467.704509	30567.736174	30.714791
468.011543	30621.717164	30.719808
468.772209	30662.956984	30.724826
468.919393	30726.123000	30.729844
469.801825	30774.311881	30.734861
470.442684	30813.010157	30.739879
470.761203	30868.150977	30.744896
471.181358	30904.280042	30.749914
471.662382	30966.375931	30.754932
471.800067	31014.511827	30.759949
472.597968	31051.020474	30.764967
472.543503	31114.890029	30.769984
473.010638	31166.849236	30.775002
473.814937	31232.056993	30.780020
474.247181	31284.747934	30.785037
474.729456	31333.127498	30.790055
475.120006	31400.855579	30.795072
475.457815	31446.296866	30.800090
476.343628	31500.932678	30.805108
476.688515	31552.127646	30.810125
477.314903	31606.557401	30.815143
477.582867	31659.790862	30.820160
478.610994	31706.737284	30.825178
478.638976	31754.924883	30.830196
479.177903	31804.015722	30.835213
479.844546	31862.724079	30.840231
479.946272	31907.937386	30.845248
480.441790	31965.548022	30.850266
480.845047	32021.561874	30.855284
481.233692	32072.688033	30.860301
481.799918	32126.334273	30.865319
481.985929	32161.403501	30.870336
482.327411	32223.694111	30.875354
482.705943	32269.676626	30.880372
483.162401	32324.745605	30.885389
483.798983	32390.960292	30.890407
484.409255	32439.621496	30.895424
484.964627	32496.615053	30.900442
485.277661	32563.634749	30.905460
485.621557	32618.761102	30.910477
486.046303	32678.865689	30.915495
486.681538	32735.783726	30.920512
487.368576	32790.030441	30.925530
487.889265	32830.172841	30.930548
488.620323	32886.829435	30.935565
489.616922	32942.946986	30.940583
490.009358	32998.120145	30.945600
490.052917	33040.787109	30.950618
490.677483	33098.859728	30.955636
491.328164	33141.839982	30.960653
491.811676	33200.103460	30.965671
492.051649	33252.440810	30.970688
492.604869	33302.659887	30.975706
493.086702	33366.512128	30.980724
493.770189	33410.667684	30.985741
494.342290	33461.720239	30.990759
494.312190	33511.064439	30.995776
495.069504	33556.135816	31.000794
495.400067	33626.059514	31.005812
495.852701	33689.700028	31.010829
496.637630	33737.569224	31.015847
496.930796	33803.218029	31.020864
497.621227	33857.991252	31.025882
498.245339	33915.198909	31.030900
498.730354	33972.338222	31.035917
499.403115	34016.945126	31.040935
499.807673	34071.387585	31.045952
500.558575	34116.616064	31.050970
500.881678	34175.149058	31.055988
501.358597	34220.252667	31.061005
502.054591	34266.787472	31.066023
502.421914	34337.345297	31.071040
502.657209	34370.564844	31.076058
503.288963	34429.180221	31.081076
503.795084	34494.515574	31.086093
504.212047	34551.295649	31.091111
504.450744	34609.916593	31.096128
504.976132	34665.741948	31.101146
505.302252	34728.675014	31.106164
505.746755	34780.045905	31.111181
506.629392	34838.154176	31.116199
506.932552	34894.610193	31.121216
507.601751	34965.944241	31.126234
508.080077	35027.344874	31.131252
508.411880	35092.076950	31.136269
509.001938	35146.558328	31.141287
509.601277	35208.737958	31.146304
510.366524	35275.494410	31.151322
510.716823	35331.246638	31.156340
511.407425	35376.096991	31.161357
511.893000	35419.173154	31.166375
512.626529	35484.894275	31.171392
513.109734	35547.084801	31.176410
513.630385	35595.895709	31.181428
513.670029	35651.387841	31.186445
514.054367	35717.647159	31.191463
514.469500	35779.322740	31.196480
515.096437	35840.991950	31.201498
515.563451	35900.371501	31.206516
516.207899	35956.632498	31.211533
516.867886	36004.231803	31.216551
517.345528	36063.193585	31.221568
517.769595	36112.785546	31.226586
518.061949	36163.093665	31.231604
518.602992	36229.344772	31.236621
518.862749	36278.172236	31.241639
519.373148	36343.504186	31.246656
519.623013	36413.559451	31.251674
520.111695	36478.526253	31.256692
520.552054	36544.719418	31.261709
520.857215	36619.945050	31.266727
521.729455	36692.338058	31.271744
522.138771	36760.140313	31.276762
522.824217	36830.636506	31.281780
523.255748	36904.299237	31.286797
523.778499	36981.336632	31.291815
524.489747	37048.427365	31.296832
524.673000	37117.994591	31.301850
525.739905	37181.845911	31.306868
526.307719	37256.052484	31.311885
527.052029	37314.822846	31.316903
527.879191	37376.214944	31.321920
528.554425	37440.785164	31.326938
528.884218	37493.435714	31.331956
529.125008	37553.268380	31.336973
529.965888	37620.611251	31.341991
530.155773	37689.261189	31.347008
530.753107	37758.443733	31.352026
531.507114	37807.673428	31.357044
532.090060	37884.745774	31.362061
532.724885	37929.933651	31.367079
532.705168	38008.024482	31.372096
533.380943	38077.886474	31.377114
534.165966	38138.540139	31.382132
534.488409	38210.345194	31.387149
534.946930	38266.205435	31.392167
535.238808	38339.685640	31.397184
535.978599	38416.087339	31.402202
536.344350	38484.038988	31.407220
536.697077	38562.926012	31.412237
537.779744	38628.619904	31.417255
538.281714	38699.302051	31.422272
538.429036	38770.219800	31.427290
539.469648	38840.131787	31.432308
539.606161	38914.470069	31.437325
540.512515	38973.256941	31.442343
540.961482	39047.140159	31.447360
541.030579	39119.947011	31.452378
541.979963	39194.508833	31.457396
542.030620	39265.015227	31.462413
542.881808	39347.086934	31.467431
543.413209	39411.283941	31.472448
543.857189	39496.737718	31.477466
544.738983	39559.172953	31.482484
544.897983	39637.209710	31.487501
545.361936	39714.969173	31.492519
546.182102	39787.269561	31.497536
546.788676	39864.311700	31.502554
547.364521	39928.392718	31.507572
547.397453	40004.479117	31.512589
548.277550	40082.957363	31.517607
548.708886	40148.868505	31.522624
549.033888	40233.168033	31.527642
549.773897	40308.864298	31.532660
549.960609	40385.245687	31.537677
551.209820	40459.397018	31.542695
551.860831	40536.024310	31.547712
552.350655	40612.700643	31.552730
552.921324	40648.654117	31.557748
553.972193	40722.855063	31.562765
554.882202	40773.029786	31.567783
555.467063	40818.697122	31.572800
555.955959	40866.555299	31.577818
556.724059	40917.820780	31.582836
557.185310	40982.928219	31.587853
557.405320	41030.316713	31.592871
557.768810	41099.216003	31.597888
558.246594	41146.319161	31.602906
558.723916	41210.607191	31.607924
559.085458	41285.344108	31.612941
559.465519	41344.983160	31.617959
560.142705	41421.849744	31.622976
560.533728	41485.048157	31.627994
561.309113	41544.991894	31.633012
561.683723	41622.180769	31.638029
562.119260	41696.029574	31.643047
562.960286	41768.864684	31.648064
562.928269	41839.836599	31.653082
563.816350	41918.674957	31.658100
564.119962	41994.630206	31.663117
564.693108	42071.062118	31.668135
565.583711	42148.335283	31.673152
566.137850	42226.529311	31.678170
566.653959	42308.420271	31.683188
567.235837	42383.478821	31.688205
567.737148	42466.992382	31.693223
568.914269	42537.126430	31.698240
568.953800	42617.313854	31.703258
569.607175	42693.356271	31.708276
569.940777	42774.300809	31.713293
570.594474	42853.222921	31.718311
571.372559	42923.395935	31.723328
571.703729	43008.673198	31.728346
572.203490	43085.437127	31.733364
572.766652	43168.242800	31.738381
573.549037	43252.240699	31.743399
574.294810	43337.147926	31.748416
575.027853	43407.901634	31.753434
575.677290	43476.027000	31.758452
576.031601	43561.625003	31.763469
576.392781	43633.135538	31.768487
577.137824	43711.648436	31.773504
577.399334	43797.666959	31.778522
578.202432	43878.166241	31.783540
578.988097	43956.117818	31.788557
579.559232	44032.163533	31.793575
580.381994	44110.090686	31.798592
580.864583	44179.471158	31.803610
581.767834	44243.803588	31.808628
582.327250	44336.020234	31.813645
582.347299	44393.723792	31.818663
583.113184	44468.548872	31.823680
583.677032	44545.576617	31.828698
584.193977	44628.055459	31.833716
584.923167	44710.480667	31.838733
585.334038	44799.560602	31.843751
585.575357	44872.664848	31.848768
586.401477	44943.955239	31.853786
587.057902	45026.213897	31.858804
587.724822	45106.980942	31.863821
588.189621	45193.269118	31.868839
588.616901	45267.585017	31.873856
589.184008	45344.508174	31.878874
590.157599	45423.495718	31.883892
590.603454	45507.448880	31.888909
591.355594	45587.638760	31.893927
591.937438	45651.050349	31.898944
591.995350	45725.334351	31.903962
592.829656	45793.396616	31.908980
593.637097	45867.920490	31.913997
593.899705	45945.922573	31.919015
594.725014	46023.150033	31.924032
594.883803	46109.928703	31.929050
595.508481	46181.446532	31.934068
596.071260	46266.087896	31.939085
596.877260	46343.619827	31.944103
597.530743	46414.082337	31.949120
597.876783	46507.974211	31.954138
599.106674	46571.967064	31.959156
599.230275	46655.568109	31.964173
599.766890	46737.137303	31.969191
600.766385	46813.792987	31.974208
601.148052	46913.740396	31.979226
601.914288	46984.656904	31.984244
602.437567	47067.559084	31.989261
602.949818	47134.201636	31.994279
603.973842	47208.297194	31.999296
604.211540	47299.902671	32.004314
604.826204	47378.970358	32.009332
605.478778	47474.549982	32.014349
606.091317	47552.361986	32.019367
606.800357	47624.502905	32.024384
607.293956	47717.826989	32.029402
607.956864	47796.806356	32.034420
608.483592	47882.038800	32.039437
609.124443	47967.874859	32.044455
609.882660	48047.480559	32.049472
610.294128	48153.214665	32.054490
611.075961	48210.813595	32.059508
611.727362	48305.652368	32.064525
611.948439	48394.771203	32.069543
612.907805	48472.002345	32.074560
613.112088	48562.078412	32.079578
613.935669	48642.244231	32.084596
614.867416	48743.572553	32.089613
615.057492	48827.806952	32.094631
615.566216	48906.582721	32.099648
616.146430	49000.779873	32.104666
617.155950	49087.700126	32.109684
618.121154	49174.703886	32.114701
618.208709	49265.569949	32.119719
619.363341	49349.549451	32.124736
619.834005	49432.066439	32.129754
620.538521	49523.005521	32.134772
621.179791	49603.322348	32.139789
622.043903	49677.690828	32.144807
622.838847	49758.576642	32.149824
623.396665	49827.681266	32.154842
623.921759	49913.873669	32.159860
624.707921	49991.272226	32.164877
625.174681	50066.604751	32.169895
626.101303	50147.628371	32.174912
626.271978	50225.745367	32.179930
626.873488	50303.908376	32.184948
627.523130	50391.272986	32.189965
627.968930	50480.446563	32.194983
628.887087	50563.276667	32.200000
629.014521	50643.041611	32.205018
629.567243	50728.225646	32.210036
630.326200	50815.030917	32.215053
630.752700	50905.605600	32.220071
631.582639	50991.651440	32.225088
632.284632	51068.566086	32.230106
632.747150	51157.086279	32.235124
633.507331	51243.501656	32.240141
633.837782	51317.765671	32.245159
634.995465	51391.056390	32.250176
635.393742	51471.263262	32.255194
636.152026	51533.837883	32.260212
637.111788	51612.938779	32.265229
637.278793	51708.806160	32.270247
637.890023	51773.591453	32.275264
638.523861	51870.885936	32.280282
638.909166	51957.312737	32.285300
640.041776	52033.749523	32.290317
640.231041	52124.233305	32.295335
641.149996	52200.522849	32.300352
641.624216	52296.651938	32.305370
642.237326	52384.230614	32.310388
642.880769	52467.319588	32.315405
643.317401	52558.611027	32.320423
644.225299	52650.880017	32.325440
644.919823	52744.643941	32.330458
644.987267	52833.837197	32.335476
645.488359	52921.771613	32.340493
645.960094	53025.371629	32.345511
647.293419	53112.379810	32.350528
648.001863	53220.938711	32.355546
648.889989	53310.706150	32.360564
650.105883	53389.471941	32.365581
650.316965	53485.669334	32.370599
651.371668	53561.152148	32.375616
651.931385	53651.556600	32.380634
652.451046	53749.498478	32.385652
653.286250	53833.351310	32.390669
653.845096	53913.718664	32.395687
654.826780	53989.234152	32.400704
654.968776	54081.402683	32.405722
655.694624	54167.650413	32.410740
656.630580	54253.225747	32.415757
656.986353	54340.122897	32.420775
657.709983	54418.538238	32.425792
658.115927	54508.839388	32.430810
658.814177	54602.339987	32.435828
659.501747	54692.974539	32.440845
660.069980	54790.698815	32.445863
660.684534	54877.005964	32.450880
661.706005	54975.085916	32.455898
662.242715	55058.298344	32.460916
663.076333	55144.955884	32.465933
663.500984	55251.930300	32.470951
664.272740	55331.131089	32.475968
664.938290	55430.188204	32.480986
665.606430	55521.322599	32.486004
666.459583	55602.267448	32.491021
666.860491	55692.871831	32.496039
667.501905	55788.965248	32.501056
668.103849	55881.615953	32.506074
668.343861	55977.580721	32.511092
669.652795	56062.925452	32.516109
670.343882	56161.596623	32.521127
670.880845	56252.320110	32.526144
671.719741	56346.905164	32.531162
672.284864	56435.963138	32.536180
673.052559	56529.872133	32.541197
673.751224	56619.167930	32.546215
674.522118	56700.074012	32.551232
675.377342	56797.653448	32.556250
675.379423	56893.200715	32.561268
676.508468	56968.235769	32.566285
677.030580	57064.841625	32.571303
677.362897	57144.760449	32.576320
678.132409	57236.915949	32.581338
678.510177	57328.043459	32.586356
679.373179	57412.431424	32.591373
679.462147	57512.289260	32.596391
680.064107	57587.856017	32.601408
680.620725	57703.781804	32.606426
681.536398	57809.911779	32.611444
682.415567	57893.692521	32.616461
683.109848	57999.626278	32.621479
683.717647	58104.481722	32.626496
684.583754	58211.595129	32.631514
685.306741	58298.392196	32.636532
686.634646	58375.067922	32.641549
687.250866	58469.908407	32.646567
687.712963	58552.768728	32.651584
688.977221	58645.196595	32.656602
689.195472	58744.565331	32.661620
689.910164	58819.460966	32.666637
690.515530	58921.319552	32.671655
691.334079	59009.904876	32.676672
691.977980	59110.879705	32.681690
692.521399	59215.163936	32.686708
693.245574	59306.944715	32.691725
693.728328	59419.714105	32.696743
694.232080	59512.202068	32.701760
694.904297	59609.370524	32.706778
695.450750	59731.496372	32.711796
696.599425	59825.218973	32.716813
696.980999	59928.111778	32.721831
697.531876	60035.539791	32.726848
698.158290	60133.742100	32.731866
698.595229	60250.770411	32.736884
699.733289	60360.454046	32.741901
700.367425	60480.124294	32.746919
701.054782	60594.275749	32.751936
701.935014	60686.706940	32.756954
702.400605	60801.983175	32.761972
703.306478	60903.625233	32.766989
704.024601	61018.589252	32.772007
705.166749	61123.580787	32.777024
705.681441	61233.669151	32.782042
706.198496	61351.872422	32.787060
707.349984	61434.087264	32.792077
708.181270	61544.997180	32.797095
708.780285	61643.780153	32.802112
709.969406	61737.397528	32.807130
710.830860	61847.147561	32.812148
711.539859	61932.907193	32.817165
712.687031	62034.053718	32.822183
713.021386	62119.983453	32.827200
713.975197	62209.312601	32.832218
714.872551	62300.901441	32.837236
715.351990	62388.533753	32.842253
716.172374	62465.094015	32.847271
716.613239	62569.052255	32.852288
717.609152	62647.322280	32.857306
718.103493	62743.302728	32.862324
718.749031	62832.685524	32.867341
719.607420	62917.843170	32.872359
720.060440	63016.694845	32.877376
721.043444	63105.587000	32.882394
721.371005	63200.560595	32.887412
722.004001	63295.831815	32.892429
722.748425	63396.874650	32.897447
723.314040	63499.262184	32.902464
724.276234	63591.844759	32.907482
724.298299	63696.705892	32.912500
725.266567	63791.949336	32.917517
725.574201	63880.608760	32.922535
726.501329	63979.570089	32.927552
727.329069	64086.082590	32.932570
727.452952	64185.809635	32.937588
728.442004	64294.445629	32.942605
729.271477	64396.907843	32.947623
729.851489	64488.091153	32.952640
730.353170	64600.247781	32.957658
731.189190	64710.586275	32.962676
731.956840	64821.202131	32.967693
732.898020	64925.683870	32.972711
733.628573	65034.530807	32.977728
734.610475	65145.410107	32.982746
735.163735	65245.121938	32.987764
735.958923	65345.281022	32.992781
736.561155	65454.581199	32.997799
737.279325	65569.722523	33.002816
738.328230	65666.105456	33.007834
738.712639	65775.291590	33.012852
739.256017	65892.081806	33.017869
740.009288	66002.118481	33.022887
740.477561	66126.982073	33.027904
741.300337	66236.648198	33.032922
742.132820	66366.377428	33.037940
742.817846	66476.510067	33.042957
743.883010	66594.134672	33.047975
744.492632	66712.473644	33.052992
745.653526	66812.592067	33.058010
746.686945	66935.729909	33.063028
747.112948	67045.851442	33.068045
748.209697	67159.080506	33.073063
748.585304	67274.755652	33.078080
749.601702	67371.006468	33.083098
750.240848	67492.392055	33.088116
751.131710	67595.744993	33.093133
752.103335	67719.005133	33.098151
752.606864	67824.477756	33.103168
753.508754	67936.617926	33.108186
753.851079	68049.072369	33.113204
755.218778	68159.265521	33.118221
756.090043	68258.231215	33.123239
756.651193	68371.106431	33.128256
757.920720	68471.790171	33.133274
758.713122	68581.562140	33.138292
759.786364	68686.635235	33.143309
760.615391	68763.280622	33.148327
761.270256	68866.849498	33.153344
761.966215	68962.635804	33.158362
762.772596	69054.863870	33.163380
762.757685	69170.601314	33.168397
763.831942	69270.815348	33.173415
764.503260	69384.246810	33.178432
765.430091	69489.948712	33.183450
765.888596	69588.084728	33.188468
766.308515	69698.221176	33.193485
767.186074	69806.012868	33.198503
767.821119	69922.513270	33.203520
768.736977	70033.176521	33.208538
769.402407	70144.988151	33.213556
770.321959	70268.815559	33.218573
770.844328	70369.233422	33.223591
771.661991	70488.823824	33.228608
772.453789	70600.825635	33.233626
772.994034	70720.475799	33.238644
773.580358	70836.647838	33.243661
774.587090	70962.058224	33.248679
775.281550	71073.509547	33.253696
776.391029	71174.649904	33.258714
776.556067	71293.347268	33.263732
777.259876	71411.317707	33.268749
778.019220	71521.262125	33.273767
778.511336	71649.132640	33.278784
779.582040	71756.181506	33.283802
780.813807	71863.090497	33.288820
781.645948	71982.781739	33.293837
782.599293	72080.841215	33.298855
782.947105	72209.130939	33.303872
783.863194	72318.143036	33.308890
784.654100	72425.184545	33.313908
785.760380	72551.466749	33.318925
786.548743	72656.929021	33.323943
787.041120	72776.598597	33.328960
787.833505	72881.264567	33.333978
788.743912	73004.217755	33.338996
789.207363	73123.337578	33.344013
790.174875	73235.899603	33.349031
790.422657	73375.885905	33.354048
791.287221	73486.436396	33.359066
792.017184	73614.886394	33.364084
792.678298	73746.700034	33.369101
793.887570	73873.270192	33.374119
794.618812	74007.653888	33.379136
795.272751	74122.953559	33.384154
796.564716	74263.203188	33.389172
797.100803	74392.018650	33.394189
798.004313	74516.214721	33.399207
798.580340	74649.907113	33.404224
799.279608	74778.767485	33.409242
800.323126	74901.589325	33.414260
800.836045	75036.363260	33.419277
802.198291	75166.514050	33.424295
802.818323	75300.709096	33.429312
803.847706	75427.355967	33.434330
804.628930	75542.819225	33.439348
805.687245	75676.292822	33.444365
806.819909	75794.248016	33.449383
807.620775	75925.488937	33.454400
808.027006	76035.242692	33.459418
809.257953	76162.012322	33.464436
809.842284	76285.278263	33.469453
811.048192	76400.163649	33.474471
811.201570	76520.580215	33.479488
811.852852	76647.713999	33.484506
812.805109	76783.450713	33.489524
813.378973	76933.335467	33.494541
814.262706	77044.855858	33.499559
814.889179	77188.124495	33.504576
815.577103	77330.605986	33.509594
816.813321	77453.650663	33.514612
817.633890	77591.665689	33.519629
818.538721	77727.194685	33.524647
819.268646	77864.726730	33.529664
819.965271	77981.235067	33.534682
821.007395	78108.312735	33.539700
821.421156	78253.678987	33.544717
822.472046	78374.703803	33.549735
823.239246	78524.067752	33.554752
823.629320	78656.449045	33.559770
825.025670	78780.360163	33.564788
825.730789	78929.079281	33.569805
826.877072	79049.389937	33.574823
827.818747	79184.719353	33.579840
828.318263	79324.569226	33.584858
829.336552	79448.097403	33.589876
830.074903	79576.233017	33.594893
831.339141	79694.509915	33.599911
831.915326	79813.426060	33.604928
832.509127	79929.537785	33.609946
833.420701	80050.101334	33.614964
833.912982	80176.579485	33.619981
835.003073	80289.473703	33.624999
836.041866	80411.738724	33.630016
836.563137	80537.587898	33.635034
837.625695	80655.118809	33.640052
838.468931	80783.174429	33.645069
839.547807	80905.897294	33.650087
840.476268	81022.016344	33.655104
841.126651	81143.982598	33.660122
841.826680	81267.193814	33.665140
842.727947	81399.291843	33.670157
843.718439	81511.544439	33.675175
844.504352	81643.789464	33.680192
844.685582	81780.348160	33.685210
845.516273	81912.884682	33.690228
846.078870	82056.403863	33.695245
847.067793	82190.225359	33.700263
847.654242	82328.472754	33.705280
848.327959	82482.382644	33.710298
849.405938	82631.981984	33.715316
850.167406	82780.552797	33.720333
851.042647	82922.665702	33.725351
851.794849	83076.471760	33.730368
852.499652	83235.493233	33.735386
853.300381	83383.277033	33.740404
854.361431	83545.196245	33.745421
855.312099	83691.616087	33.750439
856.078814	83839.098458	33.755456
856.819851	84016.997591	33.760474
857.864670	84157.938758	33.765492
858.740954	84317.059643	33.770509
859.407873	84466.201119	33.775527
860.405270	84625.474963	33.780544
861.702070	84783.137770	33.785562
862.849653	84929.229319	33.790580
863.811900	85075.985081	33.795597
864.694329	85221.521220	33.800615
865.939776	85363.980409	33.805632
866.631192	85499.464778	33.810650
867.619387	85648.225533	33.815668
868.351214	85796.162777	33.820685
869.128245	85939.183711	33.825703
870.098341	86078.117986	33.830720
870.617424	86229.762839	33.835738
871.557462	86377.378365	33.840756
872.434733	86523.265212	33.845773
873.078988	86677.986328	33.850791
874.122395	86825.410470	33.855808
874.841866	86982.019374	33.860826
875.542769	87139.670087	33.865844
875.967864	87298.189970	33.870861
877.375538	87450.809679	33.875879
878.121973	87616.694449	33.880896
878.650120	87772.770772	33.885914
879.579401	87934.040129	33.890932
880.657894	88103.973801	33.895949
881.667107	88253.424789	33.900967
882.432660	88417.635237	33.905984
883.081356	88582.695065	33.911002
884.340852	88738.416596	33.916020
885.179263	88899.448145	33.921037
885.899993	89054.716532	33.926055
887.170760	89225.145446	33.931072
887.694554	89384.504729	33.936090
888.630955	89532.109101	33.941108
889.159686	89683.755729	33.946125
890.372090	89833.860291	33.951143
891.448657	89987.993948	33.956160
891.987504	90140.205030	33.961178
892.955051	90294.137190	33.966196
893.538867	90441.400435	33.971213
894.459056	90600.797363	33.976231
895.665032	90769.767260	33.981248
896.324644	90926.159127	33.986266
897.243500	91085.679758	33.991284
897.886249	91248.790991	33.996301
899.129267	91414.759643	34.001319
899.850270	91560.583227	34.006336
901.136086	91722.667542	34.011354
902.182557	91878.501802	34.016372
902.907960	92051.920548	34.021389
903.986874	92196.385194	34.026407
905.092545	92354.041768	34.031424
905.862088	92518.976048	34.036442
907.038759	92686.787153	34.041460
907.984291	92843.517717	34.046477
908.656725	92992.838904	34.051495
909.600734	93158.387973	34.056512
910.176636	93326.410312	34.061530
911.287306	93475.200101	34.066548
911.619230	93648.296561	34.071565
912.698939	93812.903649	34.076583
913.580796	93988.228202	34.081600
914.736788	94156.192154	34.086618
915.850364	94334.310113	34.091636
916.849411	94511.403945	34.096653
917.535138	94683.791106	34.101671
918.802713	94835.576100	34.106688
919.579304	95013.121717	34.111706
920.401634	95180.793370	34.116724
921.378907	95355.080286	34.121741
922.221610	95532.074408	34.126759
923.335620	95695.188421	34.131776
924.062167	95868.165838	34.136794
924.998608	96039.483076	34.141812
926.032108	96214.190898	34.146829
927.034812	96380.638307	34.151847
928.413017	96532.288939	34.156864
929.423775	96709.333411	34.161882
930.286478	96881.358634	34.166900
931.048421	97044.305501	34.171917
932.112568	97216.831514	34.176935
933.303758	97365.289823	34.181952
934.052604	97536.236960	34.186970
935.202441	97702.225860	34.191988
936.046225	97863.512426	34.197005
936.603814	98041.970577	34.202023
937.790509	98204.994194	34.207040
938.387124	98386.727453	34.212058
939.265503	98549.601657	34.217076
940.214714	98722.492595	34.222093
940.748840	98902.524378	34.227111
941.947459	99073.357145	34.232128
942.659038	99260.180145	34.237146
943.812170	99436.998933	34.242164
944.408943	99606.022856	34.247181
945.202432	99794.596220	34.252199
946.202108	99976.742917	34.257216
946.826507	100169.531613	34.262234
947.720855	100349.995416	34.267252
949.035934	100542.324724	34.272269
949.952129	100727.485118	34.277287
951.398161	100891.224061	34.282304
951.863975	101069.117405	34.287322
952.539464	101233.625211	34.292340
954.023979	101411.681972	34.297357
954.267104	101599.435305	34.302375
955.306429	101773.338906	34.307392
956.173797	101965.246413	34.312410
957.347160	102146.949488	34.317428
958.355877	102318.576268	34.322445
959.391612	102504.059070	34.327463
960.728299	102668.542931	34.332480
961.429293	102852.222089	34.337498
962.631546	103032.407128	34.342516
963.482019	103217.577442	34.347533
964.550426	103411.767259	34.352551
965.161459	103587.881290	34.357568
966.236441	103764.749371	34.362586
967.208114	103955.058943	34.367604
968.173473	104139.463428	34.372621
968.975589	104333.862434	34.377639
970.667065	104516.725064	34.382656
971.572642	104696.609780	34.387674
972.184803	104886.624627	34.392692
973.371816	105083.378162	34.397709
974.137809	105268.944342	34.402727
975.082859	105446.250582	34.407744
976.223613	105642.699369	34.412762
977.094531	105826.618499	34.417780
978.559542	106008.933769	34.422797
979.333057	106209.056797	34.427815
980.649044	106379.507271	34.432832
981.983363	106573.220851	34.437850
983.034096	106751.721618	34.442868
984.249662	106932.944656	34.447885
984.947111	107108.542589	34.452903
985.801485	107284.799693	34.457920
986.815612	107475.887782	34.462938
988.175906	107656.965241	34.467956
988.973041	107836.946379	34.472973
989.606656	108013.992034	34.477991
990.664766	108193.514543	34.483008
991.564687	108379.435154	34.488026
992.230339	108564.357158	34.493044
993.476511	108760.697751	34.498061
994.185211	108957.027198	34.503079
995.355451	109149.786092	34.508096
996.036780	109348.048146	34.513114
997.032207	109552.580196	34.518132
998.121002	109748.434707	34.523149
998.730209	109936.934711	34.528167
999.967569	110144.065907	34.533184
1000.948064	110356.181034	34.538202
1001.491082	110551.840164	34.543220
1002.864201	110757.902333	34.548237
1003.650350	110965.329657	34.553255
1004.807595	111161.930465	34.558272
1005.614938	111375.374186	34.563290
1006.510999	111581.812718	34.568308
1008.028081	111794.154520	34.573325
1008.787494	112005.951701	34.578343
1009.746191	112202.567473	34.583360
1010.872663	112412.331098	34.588378
1011.696805	112625.731161	34.593396
1012.785691	112832.692017	34.598413
1013.655016	113050.103562	34.603431
1014.432841	113252.267191	34.608448
1015.345822	113478.973107	34.613466
1016.273356	113694.872648	34.618484
1017.607430	113896.518453	34.623501
1018.191478	114107.550026	34.628519
1019.634461	114296.905263	34.633536
1020.601695	114509.105457	34.638554
1021.373030	114715.385418	34.643572
1022.717762	114915.960057	34.648589
1023.277802	115134.515871	34.653607
1024.456116	115338.756944	34.658624
1025.682468	115549.668078	34.663642
1026.515341	115761.532593	34.668660
1027.999524	115961.128877	34.673677
1028.788874	116190.411121	34.678695
1030.328373	116387.036717	34.683712
1031.092601	116588.441331	34.688730
1032.112471	116807.757781	34.693748
1033.543573	117011.551202	34.698765
1034.128309	117230.157259	34.703783
1035.474506	117439.605772	34.708800
1036.191198	117647.436665	34.713818
1037.351106	117855.892753	34.718836
1038.831961	118058.773261	34.723853
1039.683587	118276.050968	34.728871
1041.521388	118479.509051	34.733888
1042.211986	118679.737003	34.738906
1043.550278	118897.585280	34.743924
1044.495632	119095.037279	34.748941
1045.107208	119297.930726	34.753959
1046.209626	119514.796318	34.758976
1047.115236	119727.552704	34.763994
1048.327769	119948.381998	34.769012
1049.651900	120142.991073	34.774029
1050.537146	120367.856279	34.779047
1051.644826	120571.196294	34.784064
1052.785388	120789.813781	34.789082
1053.774533	120999.182519	34.794100
1055.032763	121199.575013	34.799117
1055.747173	121423.462887	34.804135
1057.075007	121627.331491	34.809152
1058.267782	121831.996786	34.814170
1059.411634	122053.094183	34.819188
1060.783978	122246.239451	34.824205
1061.746117	122456.560813	34.829223
1063.044571	122669.793411	34.834240
1064.051052	122865.284114	34.839258
1064.578812	123078.127345	34.844276
1065.985149	123287.582962	34.849293
1066.553183	123513.982034	34.854311
1067.697789	123726.094476	34.859328
1068.821805	123934.181958	34.864346
1069.363526	124169.004955	34.869364
1070.887395	124380.970753	34.874381
1071.202712	124619.319684	34.879399
1072.191664	124830.946110	34.884416
1073.658547	125056.980416	34.889434
1074.470852	125280.387093	34.894452
1075.859930	125506.108130	34.899469
1076.738155	125745.564371	34.904487
1077.653213	125965.182522	34.909504
1078.601862	126205.112379	34.914522
1079.908868	126441.182894	34.919540
1081.211999	126669.575616	34.924557
1082.326674	126892.703517	34.929575
1083.332790	127125.001539	34.934592
1084.755365	127357.815588	34.939610
1085.354606	127588.676109	34.944628
1086.371096	127808.341551	34.949645
1087.274965	128045.973953	34.954663
1089.015135	128274.154463	34.959680
1089.844903	128489.787139	34.964698
1090.627029	128707.533170	34.969716
1092.002136	128920.303108	34.974733
1093.283975	129135.688232	34.979751
1094.376392	129356.239435	34.984768
1095.443282	129565.389000	34.989786
1096.556787	129797.283913	34.994804
1098.093615	130003.937929	34.999821
1099.089472	130211.734664	35.004839
1100.225448	130430.980770	35.009856
1101.634122	130634.694117	35.014874
1102.729143	130840.881579	35.019892
1104.135106	131045.688139	35.024909
1105.430408	131265.243356	35.029927
1105.802698	131485.345427	35.034944
1107.122703	131686.925384	35.039962
1108.035286	131908.272174	35.044980
1108.997669	132123.058829	35.049997
1110.094556	132349.385285	35.055015
1111.013335	132578.797708	35.060032
1111.876379	132796.964506	35.065050
1112.806201	133034.871467	35.070068
1113.930057	133261.973229	35.075085
1115.326492	133505.308233	35.080103
1116.553959	133735.147057	35.085120
1117.416766	133969.624012	35.090138
1118.627733	134204.577630	35.095156
1120.386994	134423.025913	35.100173
1121.179837	134666.875029	35.105191
1122.314858	134892.173685	35.110208
1123.247061	135133.328460	35.115226
1124.283472	135375.177754	35.120244
1125.179725	135610.764032	35.125261
1126.547251	135854.387769	35.130279
1127.930896	136093.522827	35.135296
1129.455797	136334.005502	35.140314
1130.289641	136571.700831	35.145332
1131.484611	136805.205310	35.150349
1132.958026	137042.012446	35.155367
1134.376113	137261.334824	35.160384
1135.973910	137489.516311	35.165402
1136.682957	137716.654343	35.170420
1138.168976	137932.356698	35.175437
1139.500474	138164.669194	35.180455
1140.501682	138388.010820	35.185472
1141.661019	138616.132988	35.190490
1142.758392	138847.170339	35.195508
1143.401596	139064.033451	35.200525
1144.382916	139301.090103	35.205543
1145.259377	139537.874127	35.210560
1146.596566	139778.450838	35.215578
1147.200412	140003.580500	35.220596
1147.948172	140265.469978	35.225613
1148.891002	140516.488566	35.230631
1150.019469	140765.792025	35.235648
1151.404182	141026.301634	35.240666
1152.459385	141288.186301	35.245684
1153.712907	141542.965035	35.250701
1154.899582	141794.802340	35.255719
1155.912417	142047.760656	35.260736
1157.709818	142298.968304	35.265754
1158.587564	142553.613709	35.270772
1160.081318	142804.520136	35.275789
1161.229420	143043.566114	35.280807
1162.122100	143309.994483	35.285824
1163.685949	143545.183908	35.290842
1164.516777	143802.712006	35.295860
1165.565126	144046.143421	35.300877
1166.836622	144288.563295	35.305895
1167.450507	144541.035056	35.310912
1168.916986	144762.490227	35.315930
1169.808803	145029.984378	35.320948
1170.858685	145273.081682	35.325965
1172.211156	145511.032940	35.330983
1173.279523	145769.842416	35.336000
1174.304199	146015.028690	35.341018
1175.257452	146278.565612	35.346036
1176.409094	146544.329027	35.351053
1178.577403	146771.603145	35.356071
1179.590294	147035.186542	35.361088
1180.797085	147284.751996	35.366106
1182.011027	147533.138602	35.371124
1182.899178	147784.954071	35.376141
1183.885027	148040.001745	35.381159
1184.934069	148305.338587	35.386176
1186.762980	148561.962851	35.391194
1187.560623	148825.734372	35.396212
1188.596954	149095.352990	35.401229
1190.124790	149351.246219	35.406247
1191.173442	149628.894693	35.411264
1192.566101	149885.612968	35.416282
1193.514744	150148.138893	35.421300
1194.760506	150415.957083	35.426317
1195.746170	150675.512888	35.431335
1197.015021	150969.990624	35.436352
1198.286162	151229.528552	35.441370
1199.547292	151501.118909	35.446388
1200.606482	151787.254181	35.451405
1202.243729	152054.702485	35.456423
1202.888602	152339.134701	35.461440
1204.033760	152615.394413	35.466458
1205.457672	152896.531374	35.471476
1206.449636	153176.143583	35.476493
1208.248312	153459.632771	35.481511
1208.898959	153748.539333	35.486528
1210.393858	154022.214803	35.491546
1211.209075	154305.695051	35.496564
1212.607475	154589.525080	35.501581
1214.029813	154868.038556	35.506599
1214.994453	155169.385314	35.511616
1216.320951	155450.785485	35.516634
1217.549112	155743.176058	35.521652
1218.789347	156035.084825	35.526669
1219.981284	156305.186029	35.531687
1221.131150	156615.988933	35.536704
1222.341598	156905.879559	35.541722
1223.612184	157206.341699	35.546740
1225.045834	157500.385922	35.551757
1226.461252	157770.333473	35.556775
1227.383462	158077.697069	35.561792
1228.872655	158357.023556	35.566810
1230.077945	158653.346655	35.571828
1231.674874	158942.909329	35.576845
1233.339372	159226.538745	35.581863
1234.146977	159504.780620	35.586880
1235.564599	159775.667433	35.591898
1236.718064	160054.502991	35.596916
1238.100787	160351.227956	35.601933
1239.813084	160636.673492	35.606951
1240.759712	160921.004166	35.611968
1242.151576	161195.583702	35.616986
1243.160605	161478.804248	35.622004
1244.106360	161765.056565	35.627021
1245.370629	162039.599374	35.632039
1246.283203	162331.113321	35.637056
1247.660162	162610.119693	35.642074
1248.680895	162886.357584	35.647092
1249.819090	163170.139297	35.652109
1251.036336	163435.653353	35.657127
1252.024721	163723.053952	35.662144
1253.133058	163989.921632	35.667162
1254.201989	164286.092272	35.672180
1255.634232	164573.146287	35.677197
1257.266790	164856.337593	35.682215
1258.462351	165146.530274	35.687232
1259.488774	165427.452868	35.692250
1260.674640	165720.188557	35.697268
1261.971070	166024.669518	35.702285
1263.382999	166307.906852	35.707303
1264.487136	166602.895090	35.712320
1266.074815	166893.364730	35.717338
1267.383614	167174.239412	35.722356
1268.759171	167477.588291	35.727373
1269.968778	167766.743147	35.732391
1271.207681	168068.025113	35.737408
1271.929576	168373.581651	35.742426
1273.131131	168686.192072	35.747444
1274.059306	169001.742819	35.752461
1275.633309	169306.670293	35.757479
1276.828154	169626.927022	35.762496
1278.049294	169939.949052	35.767514
1279.426932	170243.925591	35.772532
1280.719837	170567.281632	35.777549
1282.579169	170879.367375	35.782567
1284.056404	171194.462229	35.787584
1285.127069	171512.456081	35.792602
1286.238930	171817.032665	35.797620
1287.809358	172138.476027	35.802637
1288.988264	172447.842347	35.807655
1290.173387	172770.432322	35.812672
1291.314577	173088.628454	35.817690
1292.627513	173420.389213	35.822708
1293.463223	173745.315093	35.827725
1294.878504	174073.155094	35.832743
1296.036342	174409.072696	35.837760
1297.520785	174732.680067	35.842778
1298.974758	175061.523064	35.847796
1300.197597	175385.863336	35.852813
1301.835198	175714.007935	35.857831
1303.222552	176060.901918	35.862848
1304.596818	176390.389031	35.867866
1306.251124	176706.646532	35.872884
1307.737365	177036.297226	35.877901
1309.075975	177344.273134	35.882919
1310.610358	177675.024301	35.887936
1311.911551	177991.018437	35.892954
1313.381375	178295.272872	35.897972
1314.868980	178617.103540	35.902989
1316.297929	178930.760104	35.908007
1317.022824	179245.156718	35.913024
1318.404433	179569.638136	35.918042
1319.990354	179881.066436	35.923060
1320.614066	180204.458646	35.928077
1322.373782	180527.145067	35.933095
1323.306991	180850.883754	35.938112
1324.553355	181174.166669	35.943130
1326.151880	181505.034030	35.948148
1327.234636	181834.173688	35.953165
1328.513772	182160.516155	35.958183
1329.593136	182496.031996	35.963200
1330.926846	182832.904163	35.968218
1332.243350	183159.043634	35.973236
1333.517647	183493.797538	35.978253
1334.720908	183827.499118	35.983271
1336.218636	184156.699109	35.988288
1337.265032	184477.458865	35.993306
1338.420697	184800.030259	35.998324
1339.779034	185124.448671	36.003341
1340.647037	185457.289170	36.008359
1342.093423	185787.231113	36.013376
1343.409474	186114.023312	36.018394
1344.668941	186460.234543	36.023412
1345.774014	186802.754337	36.028429
1347.151324	187152.872663	36.033447
1348.125749	187507.311960	36.038464
1348.981638	187857.190749	36.043482
1350.791325	188206.952386	36.048500
1352.049186	188580.150760	36.053517
1353.487184	188938.990721	36.058535
1354.950740	189301.344894	36.063552
1356.245185	189670.114266	36.068570
1358.124025	190023.036426	36.073588
1359.336161	190390.072234	36.078605
1360.702185	190764.561767	36.083623
1362.066579	191118.743347	36.088640
1363.742860	191479.908188	36.093658
1365.518818	191846.326923	36.098676
1366.835474	192223.778972	36.103693
1368.153566	192586.812274	36.108711
1369.525455	192948.772557	36.113728
1370.515263	193304.615799	36.118746
1372.256818	193671.343351	36.123764
1373.677967	194051.658604	36.128781
1374.940837	194407.145853	36.133799
1376.172775	194786.278178	36.138816
1377.329058	195154.596485	36.143834
1378.805029	195536.536792	36.148852
1380.146615	195910.198984	36.153869
1381.629781	196281.567583	36.158887
1383.250098	196662.145198	36.163904
1384.495673	197037.543746	36.168922
1386.925658	197401.031134	36.173940
1388.252430	197765.692891	36.178957
1389.749070	198120.883155	36.183975
1391.191311	198494.416844	36.188992
1392.322673	198869.933715	36.194010
1393.815592	199229.866098	36.199028
1394.943000	199605.578228	36.204045
1396.513961	199984.405948	36.209063
1397.673552	200350.925089	36.214080
1398.683323	200730.789120	36.219098
1400.106749	201116.008255	36.224116
1401.466838	201489.394441	36.229133
1402.986689	201864.940042	36.234151
1404.345241	202253.972429	36.239168
1405.162225	202651.971159	36.244186
1406.945196	203032.634362	36.249204
1408.315285	203433.326748	36.254221
1409.537475	203810.620504	36.259239
1410.987152	204203.482943	36.264256
1412.522727	204602.630941	36.269274
1414.202408	204978.192013	36.274292
1415.332851	205378.299887	36.279309
1416.816095	205773.031673	36.284327
1418.783885	206162.289349	36.289344
1419.591019	206560.806326	36.294362
1421.203352	206949.529976	36.299380
1422.629524	207341.600316	36.304397
1423.828055	207739.258953	36.309415
1425.753858	208121.372318	36.314432
1426.700766	208522.898412	36.319450
1428.351605	208900.172461	36.324468
1430.297358	209283.469076	36.329485
1432.697249	209621.463709	36.334503
1434.479458	209966.875559	36.339520
1435.454853	210332.179687	36.344538
1437.218658	210676.607187	36.349556
1438.321334	211020.459562	36.354573
1439.455679	211373.387133	36.359591
1440.923037	211725.575562	36.364608
1442.036897	212099.296114	36.369626
1443.614063	212456.967729	36.374644
1444.692819	212827.852939	36.379661
1446.115884	213196.549651	36.384679
1447.712918	213570.857238	36.389696
1448.739812	213947.317649	36.394714
1449.852891	214326.127345	36.399732
1451.115272	214715.936219	36.404749
1452.133552	215101.469620	36.409767
1453.839831	215502.789645	36.414784
1454.937120	215900.123020	36.419802
1456.338727	216313.611316	36.424820
1457.497494	216710.404717	36.429837
1458.760814	217134.230809	36.434855
1460.833323	217552.236233	36.439872
1462.001198	217970.113414	36.444890
1463.421905	218418.631191	36.449908
1464.913099	218869.247441	36.454925
1466.250245	219292.537551	36.459943
1468.226500	219706.098130	36.464960
1469.253081	220132.821022	36.469978
1471.262532	220566.723639	36.474996
1472.900453	220984.434427	36.480013
1474.330644	221408.987994	36.485031
1475.644608	221827.314413	36.490048
1477.168563	222251.322555	36.495066
1478.849947	222672.741129	36.500084
1480.362998	223109.504686	36.505101
1481.622573	223540.800236	36.510119
1483.219537	223967.647752	36.515136
1484.256179	224405.917423	36.520154
1486.162659	224829.643845	36.525172
1487.598799	225280.779229	36.530189
1488.942914	225717.123644	36.535207
1490.701459	226157.211241	36.540224
1492.311710	226596.689953	36.545242
1493.929709	227028.422061	36.550260
1495.434041	227462.587450	36.555277
1497.121082	227901.804216	36.560295
1498.497525	228333.047365	36.565312
1499.906601	228773.303653	36.570330
1501.344399	229207.130455	36.575348
1502.939837	229654.140860	36.580365
1504.129092	230103.023238	36.585383
1505.997513	230525.099136	36.590400
1507.419984	230971.202673	36.595418
1509.083238	231414.397650	36.600436
1510.701910	231854.299296	36.605453
1511.969122	232301.550335	36.610471
1513.728595	232729.366057	36.615488
1514.701373	233191.045324	36.620506
1516.601495	233619.526247	36.625524
1518.219077	234075.589813	36.630541
1519.151041	234516.273145	36.635559
1520.690861	234962.115476	36.640576
1522.247169	235417.075413	36.645594
1524.155817	235857.575897	36.650612
1526.036472	236302.603639	36.655629
1527.377163	236729.000736	36.660647
1529.194784	237172.466275	36.665664
1530.376056	237608.036427	36.670682
1532.215633	238021.196315	36.675700
1533.591927	238440.428414	36.680717
1535.265614	238860.349050	36.685735
1536.904489	239271.004683	36.690752
1538.621045	239685.992113	36.695770
1539.769843	240117.432999	36.700788
1541.359373	240530.309404	36.705805
1542.982488	240940.564690	36.710823
1544.743961	241367.156945	36.715840
1546.152380	241799.777834	36.720858
1547.655563	242222.680291	36.725876
1549.056368	242653.221138	36.730893
1550.461802	243080.916976	36.735911
1552.203785	243520.471791	36.740928
1553.765868	243946.619210	36.745946
1554.976086	244392.613970	36.750964
1556.640775	244829.745255	36.755981
1557.593629	245283.404801	36.760999
1559.239414	245724.757528	36.766016
1560.700838	246183.288181	36.771034
1561.703654	246651.218043	36.776052
1563.682165	247109.639452	36.781069
1564.752246	247587.720788	36.786087
1566.263536	248053.892341	36.791104
1567.454935	248529.999057	36.796122
1569.031950	249018.845874	36.801140
1570.658577	249495.415574	36.806157
1572.493920	249992.095999	36.811175
1573.731792	250457.858608	36.816192
1575.894673	250953.393879	36.821210
1577.815976	251443.838182	36.826228
1579.198404	251932.796953	36.831245
1580.746409	252423.862775	36.836263
1582.778906	252900.470974	36.841280
1584.166778	253379.446850	36.846298
1586.220326	253865.248360	36.851316
1587.908641	254345.725053	36.856333
1589.301430	254827.978284	36.861351
1591.411574	255302.187677	36.866368
1593.218180	255778.911564	36.871386
1594.621513	256268.734130	36.876404
1596.511846	256735.867697	36.881421
1597.762491	257224.115528	36.886439
1599.799990	257688.862710	36.891456
1601.476289	258166.396695	36.896474
1603.146649	258641.366068	36.901492
1605.107264	259113.290070	36.906509
1606.307869	259595.424671	36.911527
1607.888441	260068.681691	36.916544
1609.741595	260541.487315	36.921562
1611.465482	261003.111416	36.926580
1613.645654	261475.786861	36.931597
1614.915765	261939.746668	36.936615
1616.498726	262399.310824	36.941632
1618.407499	262870.760681	36.946650
1619.791912	263342.601775	36.951668
1621.475994	263801.463010	36.956685
1622.840928	264277.828788	36.961703
1624.330206	264742.666173	36.966720
1626.453473	265207.779786	36.971738
1628.302997	265678.654052	36.976756
1629.643621	266140.289032	36.981773
1631.071294	266614.890399	36.986791
1632.545387	267079.398716	36.991808
1634.326585	267549.012865	36.996826
1635.470508	268020.865654	37.001844
1637.589956	268472.564832	37.006861
1639.174017	268944.496611	37.011879
1640.324672	269387.387528	37.016896
1641.787132	269848.516775	37.021914
1642.862438	270314.053337	37.026932
1644.519928	270777.283272	37.031949
1645.484744	271254.598590	37.036967
1647.144991	271731.569951	37.041984
1648.460570	272219.393793	37.047002
1649.816322	272711.732042	37.052020
1651.625065	273209.075401	37.057037
1652.770392	273714.199098	37.062055
1654.548059	274210.834747	37.067072
1656.153434	274726.346804	37.072090
1657.360376	275249.366661	37.077108
1659.124256	275767.390949	37.082125
1660.790577	276296.378842	37.087143
1662.556408	276828.499155	37.092160
1664.178732	277362.699624	37.097178
1665.911322	277888.370934	37.102196
1667.686690	278424.398172	37.107213
1669.226344	278963.054082	37.112231
1670.923066	279494.849586	37.117248
1672.807402	280048.788902	37.122266
1674.008014	280594.025050	37.127284
1675.884947	281129.698617	37.132301
1677.526793	281681.641370	37.137319
1679.337883	282237.339511	37.142336
1680.902390	282798.512688	37.147354
1682.410709	283359.210796	37.152372
1684.494978	283919.939142	37.157389
1686.097643	284484.275972	37.162407
1687.608925	285057.948358	37.167424
1689.645252	285622.260654	37.172442
1690.628275	286204.144663	37.177460
1692.995784	286752.420972	37.182477
1694.674324	287326.997567	37.187495
1696.660281	287890.268643	37.192512
1698.819418	288459.478247	37.197530
1700.245121	289029.492473	37.202548
1702.162953	289596.400566	37.207565
1703.701678	290161.997297	37.212583
1705.504116	290732.298103	37.217600
1707.462680	291304.907595	37.222618
1708.422658	291878.568385	37.227636
1710.626410	292451.665860	37.232653
1712.366827	293022.373416	37.237671
1714.170123	293599.138603	37.242688
1715.520238	294179.176252	37.247706
1717.021089	294764.088414	37.252724
1719.136693	295338.355476	37.257741
1720.999878	295921.271796	37.262759
1722.543003	296497.608765	37.267776
1724.649754	297065.696693	37.272794
1725.999609	297654.632250	37.277812
1728.297492	298228.473696	37.282829
1730.190630	298814.290919	37.287847
1731.898265	299386.191684	37.292864
1733.779213	299948.764900	37.297882
1735.349761	300523.374314	37.302900
1737.188329	301092.196289	37.307917
1739.036609	301670.004381	37.312935
1740.931416	302229.311747	37.317952
1742.916376	302802.773025	37.322970
1744.378244	303369.104278	37.327988
1746.633278	303934.387016	37.333005
1748.288545	304487.980949	37.338023
1750.294599	305037.754939	37.343040
1752.350930	305588.025291	37.348058
1754.041138	306135.025722	37.353076
1755.973930	306663.595568	37.358093
1757.873897	307177.767821	37.363111
1759.336782	307707.754958	37.368128
1760.908440	308220.502239	37.373146
1762.361977	308773.010875	37.378164
1764.046300	309306.151523	37.383181
1765.313172	309846.011351	37.388199
1766.941210	310391.928433	37.393216
1768.881113	310924.813359	37.398234
1770.377501	311497.079857	37.403252
1772.349203	312045.316286	37.408269
1774.103020	312592.899215	37.413287
1775.397052	313159.498664	37.418304
1777.563402	313716.833432	37.423322
1779.095467	314283.182227	37.428340
1780.909946	314855.752585	37.433357
1782.651915	315414.008343	37.438375
1784.481473	315999.086716	37.443392
1786.287465	316557.094766	37.448410
1787.916237	317146.260096	37.453428
1789.927156	317728.095131	37.458445
1791.823871	318295.444880	37.463463
1793.734799	318878.759799	37.468480
1795.787594	319451.432370	37.473498
1797.337286	320031.978667	37.478516
1799.033827	320625.979063	37.483533
1801.218997	321214.459800	37.488551
1802.803036	321790.084803	37.493568
1804.848621	322374.947376	37.498586
1806.231724	322969.156478	37.503604
1808.346084	323565.829442	37.508621
1809.824632	324152.267761	37.513639
1811.272471	324764.858056	37.518656
1813.769315	325362.543039	37.523674
1815.001234	325965.635988	37.528692
1816.975840	326579.822896	37.533709
1818.647448	327185.472028	37.538727
1820.298419	327799.598612	37.543744
1822.315140	328410.231138	37.548762
1824.317229	329024.769760	37.553780
1825.566292	329645.291026	37.558797
1827.766882	330262.627616	37.563815
1829.056524	330912.020667	37.568832
1830.832745	331528.804559	37.573850
1832.587920	332169.246394	37.578868
1834.054848	332813.308177	37.583885
1835.950282	333454.905578	37.588903
1837.653195	334100.716174	37.593920
1839.627439	334747.210708	37.598938
1841.558828	335405.001469	37.603956
1843.363052	336045.213032	37.608973
1845.493725	336709.580785	37.613991
1847.530247	337351.363172	37.619008
1850.106414	337987.337234	37.624026
1851.917427	338629.750567	37.629044
1853.761083	339271.389106	37.634061
1855.804410	339903.544005	37.639079
1857.562989	340552.034304	37.644096
1859.776457	341178.967184	37.649114
1861.758963	341830.932497	37.654132
1863.501608	342450.566222	37.659149
1865.673616	343092.305460	37.664167
1866.942051	343720.986857	37.669184
1868.688359	344355.393751	37.674202
1870.314470	345005.751608	37.679220
1871.899514	345645.955152	37.684237
1874.044624	346286.311576	37.689255
1875.736770	346918.257129	37.694272
1877.415749	347550.018749	37.699290
1879.213248	348174.747575	37.704308
1881.107313	348800.416504	37.709325
1883.023671	349433.864591	37.714343
1884.529114	350072.041360	37.719360
1886.050281	350708.531653	37.724378
1887.866185	351348.491888	37.729396
1889.714413	352004.958354	37.734413
1891.444320	352652.324341	37.739431
1893.012795	353326.530591	37.744448
1895.211608	353986.487976	37.749466
1897.209336	354643.321955	37.754484
1898.943303	355309.553039	37.759501
1901.696353	355976.189348	37.764519
1903.947302	356617.092039	37.769536
1906.791410	357259.257430	37.774554
1908.880054	357909.022960	37.779572
1910.717850	358559.530252	37.784589
1912.676151	359204.882134	37.789607
1914.279066	359859.645098	37.794624
1916.562748	360497.767962	37.799642
1918.816093	361144.385446	37.804660
1920.332555	361805.728152	37.809677
1922.251713	362450.324775	37.814695
1923.525541	363118.510712	37.819712
1925.409406	363789.781452	37.824730
1927.211623	364454.458105	37.829748
1928.926748	365129.336359	37.834765
1930.528586	365804.627525	37.839783
1931.706828	366495.020307	37.844800
1933.427566	367197.817663	37.849818
1935.224451	367906.677755	37.854836
1936.668100	368627.175633	37.859853
1938.538076	369348.299699	37.864871
1940.103570	370086.125628	37.869888
1941.853183	370817.286152	37.874906
1943.745308	371572.378698	37.879924
1945.353925	372317.787865	37.884941
1947.379255	373070.849092	37.889959
1949.198827	373844.143297	37.894976
1950.836478	374609.613746	37.899994
1953.085810	375384.908963	37.905012
1955.094461	376166.668845	37.910029
1957.492503	376937.796881	37.915047
1959.448536	377711.719795	37.920064
1961.373250	378483.576484	37.925082
1963.102682	379266.302036	37.930100
1965.163695	380048.422511	37.935117
1967.441119	380824.099034	37.940135
1968.993435	381605.506829	37.945152
1970.840825	382403.608936	37.950170
1972.970377	383195.762720	37.955188
1974.792447	383996.315807	37.960205
1976.750133	384798.044162	37.965223
1978.667409	385599.607449	37.970240
1981.153869	386395.073555	37.975258
1983.499011	387183.013421	37.980276
1985.374471	387991.496577	37.985293
1987.391367	388782.341496	37.990311
1989.127401	389584.646620	37.995328
1991.190083	390391.161782	38.000346
1993.329698	391182.585429	38.005364
1995.510296	391995.706875	38.010381
1997.638926	392788.789840	38.015399
1999.471224	393583.396799	38.020416
2001.787526	394372.605629	38.025434
2003.770207	395160.074710	38.030452
2005.968521	395937.273128	38.035469
2007.957735	396695.324567	38.040487
2009.928856	397472.926168	38.045504
2011.651605	398241.525776	38.050522
2013.533090	398997.635426	38.055540
2015.574616	399778.053949	38.060557
2017.680187	400547.898618	38.065575
2019.458202	401330.093002	38.070592
2021.511723	402106.138921	38.075610
2023.903840	402874.632624	38.080628
2025.817078	403645.921326	38.085645
2027.959480	404443.098428	38.090663
2030.076115	405224.370196	38.095680
2031.848816	406008.438767	38.100698
2034.192072	406802.804693	38.105716
2035.587230	407596.924244	38.110733
2037.405828	408397.361007	38.115751
2039.636546	409211.843230	38.120768
2041.222813	410018.199300	38.125786
2043.482405	410820.544446	38.130804
2044.823374	411645.740431	38.135821
2047.237734	412477.750923	38.140839
2048.909071	413301.828215	38.145856
2051.284630	414140.809858	38.150874
2053.642276	414957.807431	38.155892
2055.537774	415801.703964	38.160909
2057.990029	416630.740807	38.165927
2060.325179	417469.090806	38.170944
2062.234318	418309.206075	38.175962
2064.347458	419143.790061	38.180980
2065.936467	419996.692100	38.185997
2068.308288	420844.346469	38.191015
2070.319573	421693.171448	38.196032
2072.334436	422546.727727	38.201050
2074.725483	423399.534554	38.206068
2076.385615	424243.469469	38.211085
2079.105622	425112.064252	38.216103
2081.052293	425965.590362	38.221120
2082.740144	426828.750059	38.226138
2085.061044	427691.521667	38.231156
2086.712679	428561.410708	38.236173
2088.950751	429432.234921	38.241191
2091.088134	430301.272214	38.246208
2093.079055	431184.780966	38.251226
2095.477631	432059.533011	38.256244
2097.623871	432935.610478	38.261261
2100.234177	433799.581873	38.266279
2102.225752	434684.680512	38.271296
2103.727710	435560.006737	38.276314
2106.578392	436433.710889	38.281332
2108.456829	437314.071237	38.286349
2110.682129	438189.431391	38.291367
2112.606536	439071.437282	38.296384
2114.539529	439947.435942	38.301402
2116.837734	440831.386510	38.306420
2119.240885	441728.694646	38.311437
2121.083408	442612.144132	38.316455
2123.113474	443496.691385	38.321472
2125.461532	444385.451555	38.326490
2127.657241	445272.430201	38.331508
2129.601355	446163.563022	38.336525
2131.086514	447058.782352	38.341543
2133.504222	447952.900409	38.346560
2135.521171	448853.775486	38.351578
2137.726452	449743.352151	38.356596
2139.543975	450662.394336	38.361613
2141.721097	451562.825457	38.366631
2144.063755	452460.409263	38.371648
2145.619270	453347.463873	38.376666
2147.967240	454223.375952	38.381684
2149.552222	455127.545167	38.386701
2151.941655	456017.787711	38.391719
2154.030259	456890.292687	38.396736
2155.690918	457790.034967	38.401754
2158.046494	458683.505153	38.406772
2160.023403	459596.717066	38.411789
2162.208098	460508.893073	38.416807
2164.394644	461416.224865	38.421824
2166.313310	462343.073429	38.426842
2168.412077	463264.440490	38.431860
2170.244380	464201.630566	38.436877
2172.703845	465130.383428	38.441895
2174.717362	466065.484112	38.446912
2176.650022	467012.228673	38.451930
2179.098053	467954.950970	38.456948
2181.149443	468902.291847	38.461965
2183.123798	469857.583477	38.466983
2185.679319	470823.040358	38.472000
2187.966532	471779.599899	38.477018
2190.467968	472735.065727	38.482036
2192.671554	473709.074858	38.487053
2195.031040	474674.874312	38.492071
2196.937401	475639.031900	38.497088
2199.082860	476608.152108	38.502106
2201.466957	477584.001964	38.507124
2203.795188	478566.780259	38.512141
2205.660494	479545.744108	38.517159
2208.057596	480530.477344	38.522176
2209.804316	481513.345853	38.527194
2212.088311	482504.859788	38.532212
2214.758505	483502.517544	38.537229
2216.559890	484511.170239	38.542247
2219.249483	485519.216035	38.547264
2221.187733	486527.076567	38.552282
2223.504548	487537.140065	38.557300
2225.399629	488559.735328	38.562317
2227.452477	489574.320106	38.567335
2229.635309	490590.894487	38.572352
2231.510095	491611.246190	38.577370
2234.036652	492650.811498	38.582388
2236.079052	493693.119616	38.587405
2238.043873	494722.811916	38.592423
2240.520950	495769.868292	38.597440
2242.781878	496834.153071	38.602458
2244.977479	497866.292494	38.607476
2247.096615	498922.548379	38.612493
2249.110319	499981.530266	38.617511
2251.736464	501029.498553	38.622528
2254.168690	502093.272193	38.627546
2256.643231	503133.617375	38.632564
2258.907047	504205.101704	38.637581
2261.038699	505266.905540	38.642599
2263.282585	506329.731705	38.647616
2265.653294	507403.360022	38.652634
2267.723228	508455.486851	38.657652
2270.352184	509512.696893	38.662669
2272.839336	510571.272721	38.667687
2275.698237	511623.113363	38.672704
2277.998403	512683.143384	38.677722
2280.390841	513739.357556	38.682740
2282.438783	514785.578337	38.687757
2284.695288	515848.377796	38.692775
2287.229579	516901.534676	38.697792
2288.840552	517958.703613	38.702810
2291.490449	519017.594771	38.707828
2293.702136	520065.400969	38.712845
2295.527504	521109.723427	38.717863
2298.112668	522135.360502	38.722880
2299.973034	523176.614677	38.727898
2302.473921	524210.337831	38.732916
2304.771390	525236.771073	38.737933
2306.396003	526292.306743	38.742951
2309.287181	527316.385482	38.747968
2311.600765	528382.539219	38.752986
2313.701961	529418.388525	38.758004
2316.099967	530465.043198	38.763021
2317.829224	531522.206714	38.768039
2320.365339	532572.415420	38.773056
2322.741189	533645.732413	38.778074
2325.184293	534711.912524	38.783092
2327.891010	535772.887620	38.788109
2330.098233	536841.819755	38.793127
2332.416174	537903.961366	38.798144
2334.601938	538983.206478	38.803162
2336.924872	540059.127506	38.808180
2339.573189	541139.391989	38.813197
2341.470533	542229.307771	38.818215
2344.319771	543322.101950	38.823232
2346.111341	544425.096936	38.828250
2348.691538	545512.735442	38.833268
2351.316434	546623.065942	38.838285
2353.014778	547740.250222	38.843303
2355.188260	548848.114178	38.848320
2357.574663	549979.889731	38.853338
2359.790010	551093.751609	38.858356
2362.033697	552216.065239	38.863373
2364.175461	553366.756822	38.868391
2366.699794	554494.165624	38.873408
2369.039087	555641.515645	38.878426
2371.205820	556804.778734	38.883444
2373.699392	557956.530119	38.888461
2376.060529	559123.630890	38.893479
2378.530812	560269.056621	38.898496
2380.612975	561436.553480	38.903514
2383.140193	562612.615106	38.908532
2386.148885	563779.501040	38.913549
2388.316455	564948.330598	38.918567
2391.499843	566114.025571	38.923584
2394.049307	567283.788407	38.928602
2396.575174	568439.189045	38.933620
2399.210775	569595.372071	38.938637
2401.746697	570765.022912	38.943655
2404.369480	571921.048962	38.948672
2406.683324	573074.310760	38.953690
2409.068679	574244.320351	38.958708
2411.791633	575395.396633	38.963725
2413.987818	576543.343532	38.968743
2416.642100	577699.038094	38.973760
2418.943566	578867.879526	38.978778
2421.327909	580006.296526	38.983796
2424.071177	581167.524798	38.988813
2426.293383	582331.488780	38.993831
2428.735772	583488.285135	38.998848
2431.065465	584651.510529	39.003866
2433.700117	585808.557828	39.008884
2436.106509	586960.368624	39.013901
2438.197472	588129.017587	39.018919
2440.239678	589304.379402	39.023936
2442.724663	590469.027455	39.028954
2445.268830	591634.154275	39.033972
2448.314772	592804.848168	39.038989
2450.427386	593982.846924	39.044007
2452.783063	595157.131329	39.049024
2454.692387	596323.006066	39.054042
2456.992175	597478.431633	39.059060
2459.135925	598631.715572	39.064077
2461.319131	599792.842946	39.069095
2463.818314	600937.826973	39.074112
2466.155608	602117.076590	39.079130
2468.449531	603278.838850	39.084148
2470.771887	604437.775887	39.089165
2472.922409	605641.328073	39.094183
2475.661534	606814.123287	39.099200
2478.103226	608003.113111	39.104218
2480.446574	609203.304808	39.109236
2483.155005	610396.303659	39.114253
2485.328585	611593.167171	39.119271
2487.655171	612802.785378	39.124288
2490.229979	614032.091139	39.129306
2492.453901	615248.664919	39.134324
2495.178873	616476.025605	39.139341
2497.457317	617712.075001	39.144359
2499.988111	618938.244221	39.149376
2502.922870	620189.957573	39.154394
2505.017246	621425.919767	39.159412
2507.775992	622676.627581	39.164429
2509.888657	623934.294924	39.169447
2512.411052	625197.445530	39.174464
2514.618323	626470.093734	39.179482
2517.133892	627752.182795	39.184500
2519.580614	629024.088952	39.189517
2521.574829	630316.047224	39.194535
2524.018876	631633.494483	39.199552
2526.721458	632929.662337	39.204570
2529.086518	634235.512791	39.209588
2532.029138	635549.892314	39.214605
2533.893653	636888.644059	39.219623
2536.564865	638208.075075	39.224640
2539.064850	639541.140346	39.229658
2541.108736	640890.375794	39.234676
2543.825094	642242.017985	39.239693
2546.234882	643602.262643	39.244711
2548.822781	644961.499066	39.249728
2551.408518	646326.539133	39.254746
2553.680235	647686.311397	39.259764
2556.526686	649059.367447	39.264781
2558.880542	650444.331644	39.269799
2561.675234	651825.493147	39.274816
2564.571980	653215.068836	39.279834
2566.659917	654596.112834	39.284852
2569.785657	655982.971617	39.289869
2572.197478	657372.493336	39.294887
2575.077850	658768.167095	39.299904
2577.839787	660154.996203	39.304922
2580.458147	661555.495108	39.309940
2582.958308	662950.335327	39.314957
2585.139503	664334.971793	39.319975
2588.164969	665732.012630	39.324992
2590.973485	667122.715385	39.330010
2593.929983	668515.033079	39.335028
2596.891412	669890.430390	39.340045
2600.059522	671282.955654	39.345063
2602.849766	672660.765627	39.350080
2606.028143	674017.225092	39.355098
2607.951461	675383.988525	39.360116
2611.071670	676753.388134	39.365133
2613.438386	678125.097198	39.370151
2616.293764	679479.824068	39.375168
2618.775816	680845.794461	39.380186
2621.674634	682215.518872	39.385204
2623.979632	683561.241829	39.390221
2626.510939	684911.896010	39.395239
2629.230654	686240.417622	39.400256
2631.847671	687569.904585	39.405274
2634.519196	688877.888064	39.410292
2637.519426	690200.173676	39.415309
2639.815422	691513.993083	39.420327
2642.539932	692835.093340	39.425344
2645.407097	694146.001435	39.430362
2647.271977	695471.716722	39.435380
2649.741717	696798.871041	39.440397
2652.247349	698136.782146	39.445415
2654.613783	699479.175221	39.450432
2657.163999	700816.870887	39.455450
2659.625644	702184.866507	39.460468
2662.244661	703556.885110	39.465485
2664.477356	704942.776983	39.470503
2666.997417	706311.106637	39.475520
2669.516185	707692.844960	39.480538
2671.651527	709114.698266	39.485556
2674.642567	710511.807532	39.490573
2677.109867	711917.936461	39.495591
2679.636155	713351.600189	39.500608
2682.452723	714775.519289	39.505626
2684.831408	716212.832994	39.510644
2687.189495	717660.347179	39.515661
2689.655057	719115.808046	39.520679
2692.412002	720576.756202	39.525696
2695.520897	722035.016799	39.530714
2697.931045	723522.808287	39.535732
2700.984520	724990.301404	39.540749
2703.393337	726481.764125	39.545767
2705.805046	727980.617208	39.550784
2708.677818	729463.554481	39.555802
2711.187353	730976.668054	39.560820
2713.943898	732491.485226	39.565837
2716.917145	734008.996708	39.570855
2719.620108	735527.156830	39.575872
2722.691563	737044.772741	39.580890
2725.352340	738556.147482	39.585908
2728.041411	740069.551568	39.590925
2731.413258	741608.608315	39.595943
2733.990337	743122.634328	39.600960
2737.089822	744640.427740	39.605978
2739.636294	746159.647490	39.610996
2742.567732	747678.263563	39.616013
2745.651737	749199.911946	39.621031
2748.409499	750729.005693	39.626048
2750.919059	752240.938298	39.631066
2753.669319	753779.336439	39.636084
2756.428956	755312.402386	39.641101
2759.095177	756848.477603	39.646119
2761.965041	758386.673175	39.651136
2764.932870	759917.798856	39.656154
2767.524641	761458.226286	39.661172
2770.210048	762993.749232	39.666189
2773.085939	764526.026199	39.671207
2775.568801	766069.418004	39.676224
2778.916529	767611.808883	39.681242
2782.036235	769151.067524	39.686260
2785.219355	770680.756494	39.691277
2788.701592	772198.384425	39.696295
2791.464011	773722.108939	39.701312
2794.632141	775236.265350	39.706330
2797.183786	776753.993166	39.711348
2799.916540	778256.743409	39.716365
2802.581356	779771.272681	39.721383
2805.396129	781290.272140	39.726400
2808.120833	782797.582967	39.731418
2810.532674	784311.646979	39.736436
2812.965618	785800.322826	39.741453
2815.762619	787278.134584	39.746471
2818.140059	788761.447031	39.751488
2820.930397	790249.236104	39.756506
2823.770149	791743.959384	39.761524
2826.286472	793232.001177	39.766541
2829.076451	794745.992860	39.771559
2831.779005	796248.162528	39.776576
2834.119974	797756.436190	39.781594
2836.970292	799285.549147	39.786612
2839.495867	800813.988341	39.791629
2842.048189	802353.978690	39.796647
2844.457196	803915.471559	39.801664
2847.318169	805469.150014	39.806682
2850.367698	807035.503831	39.811700
2853.092085	808604.193262	39.816717
2856.059444	810187.586882	39.821735
2858.706243	811773.010570	39.826752
2861.660970	813368.957325	39.831770
2864.827478	814976.704178	39.836788
2867.357498	816574.014000	39.841805
2870.576707	818175.273065	39.846823
2873.001241	819799.075243	39.851840
2876.018772	821410.134988	39.856858
2879.001439	823048.960907	39.861876
2881.505705	824675.265566	39.866893
2884.158602	826318.895105	39.871911
2886.776060	827964.654551	39.876928
2889.804112	829627.966653	39.881946
2892.321002	831299.904924	39.886964
2895.272177	832967.006150	39.891981
2898.525085	834643.271867	39.896999
2900.760202	836334.753480	39.902016
2904.107368	838016.991425	39.907034
2906.889001	839716.400247	39.912052
2909.684544	841412.727606	39.917069
2912.905019	843112.959040	39.922087
2915.383677	844829.243633	39.927104
2918.399611	846537.195873	39.932122
2921.419022	848272.191156	39.937140
2924.434148	849993.006571	39.942157
2927.643098	851710.887973	39.947175
2930.418875	853429.241226	39.952192
2933.426186	855155.139277	39.957210
2936.420509	856886.867125	39.962228
2939.559530	858625.750511	39.967245
2942.998317	860357.592845	39.972263
2945.013689	862089.858636	39.977280
2948.341378	863822.870674	39.982298
2951.224496	865571.260573	39.987316
2953.727329	867326.669507	39.992333
2957.092799	869065.926908	39.997351
2959.944299	870819.679383	40.002368
2963.454700	872565.936478	40.007386
2966.464321	874317.088503	40.012404
2969.039412	876073.505347	40.017421
2972.121030	877815.970322	40.022439
2975.025627	879578.353803	40.027456
2978.215415	881335.716061	40.032474
2981.142084	883100.036535	40.037492
2983.741393	884860.014148	40.042509
2987.077784	886620.690826	40.047527
2989.699068	888391.185803	40.052544
2992.286938	890153.229696	40.057562
2995.434253	891929.888667	40.062580
2998.251420	893719.074943	40.067597
3001.237094	895497.645326	40.072615
3003.789874	897276.889298	40.077632
3006.708644	899035.759840	40.082650
3009.732710	900773.449642	40.087668
3012.338689	902525.120292	40.092685
3015.482311	904261.136873	40.097703
3018.428754	906021.192772	40.102720
3021.214473	907785.820449	40.107738
3024.239180	909554.081901	40.112756
3027.003295	911339.323951	40.117773
3030.021899	913106.355983	40.122791
3032.432498	914904.057396	40.127808
3035.327582	916702.339330	40.132826
3038.338029	918506.829719	40.137844
3040.946650	920330.469697	40.142861
3043.944582	922146.043730	40.147879
3047.158408	923982.751303	40.152896
3050.106164	925818.014214	40.157914
3053.128372	927671.716892	40.162932
3055.663571	929532.046213	40.167949
3058.745028	931397.098060	40.172967
3061.720487	933282.008380	40.177984
3064.653487	935160.128024	40.183002
3068.171032	937053.369982	40.188020
3071.248307	938952.986852	40.193037
3074.437334	940841.568421	40.198055
3077.303353	942757.626296	40.203072
3080.352832	944664.634417	40.208090
3083.378342	946571.327159	40.213108
3086.472683	948496.880818	40.218125
3089.604118	950424.953504	40.223143
3093.396048	952368.127685	40.228160
3096.157673	954290.224838	40.233178
3099.098430	956267.465934	40.238196
3101.933552	958261.365254	40.243213
3104.854999	960252.508358	40.248231
3107.950094	962262.873442	40.253248
3110.950055	964281.150390	40.258266
3114.197757	966304.050492	40.263284
3117.250453	968323.439704	40.268301
3120.834953	970356.183250	40.273319
3123.935775	972396.384292	40.278336
3126.893039	974407.502098	40.283354
3130.059376	976442.155719	40.288372
3133.167592	978494.710461	40.293389
3136.694671	980527.071854	40.298407
3139.568535	982572.355043	40.303424
3142.705594	984619.101130	40.308442
3145.986040	986666.548715	40.313460
3148.831539	988721.698587	40.318477
3152.397778	990758.385329	40.323495
3155.441730	992832.536877	40.328512
3158.481192	994889.216941	40.333530
3161.914522	996938.286648	40.338548
3164.560596	999017.917502	40.343565
3167.878747	1001089.102429	40.348583
3171.381736	1003151.638722	40.353600
3174.770405	1005212.374282	40.358618
3178.098519	1007269.943704	40.363636
3181.011708	1009337.299783	40.368653
3184.249601	1011397.061466	40.373671
3187.392991	1013477.394694	40.378688
3190.844058	1015541.125571	40.383706
3193.845922	1017615.400240	40.388724
3197.188679	1019680.725245	40.393741
3200.715095	1021731.428918	40.398759
3203.868209	1023809.868347	40.403776
3207.185964	1025883.933192	40.408794
3210.106322	1027931.982391	40.413812
3213.285080	1029994.497382	40.418829
3216.806020	1032011.013249	40.423847
3219.945606	1034015.282138	40.428864
3222.966414	1036026.374409	40.433882
3226.206990	1038032.653645	40.438900
3228.951726	1040059.691878	40.443917
3232.162587	1042069.917128	40.448935
3235.215477	1044100.729580	40.453952
3238.274087	1046119.434547	40.458970
3241.338576	1048150.879507	40.463988
3244.194702	1050205.284579	40.469005
3247.521018	1052256.348083	40.474023
3250.392220	1054328.263337	40.479040
3253.561642	1056399.063338	40.484058
3256.824142	1058469.742831	40.489076
3259.587500	1060568.635465	40.494093
3262.937364	1062660.390490	40.499111
3266.192578	1064770.271427	40.504128
3269.220785	1066882.449052	40.509146
3272.470442	1069001.065211	40.514164
3275.774441	1071134.286841	40.519181
3278.923252	1073262.965840	40.524199
3282.424953	1075397.750573	40.529216
3285.947733	1077551.613148	40.534234
3289.715306	1079686.400724	40.539252
3292.911974	1081837.093411	40.544269
3296.164117	1083980.807273	40.549287
3299.185762	1086144.745760	40.554304
3302.068132	1088312.241492	40.559322
3305.642804	1090499.008249	40.564340
3308.672611	1092692.430723	40.569357
3311.727811	1094873.603633	40.574375
3315.010119	1097077.520409	40.579392
3318.224244	1099284.841610	40.584410
3321.637720	1101491.799995	40.589428
3324.763834	1103716.102767	40.594445
3327.804257	1105924.357591	40.599463
3331.073514	1108166.800784	40.604480
3334.443882	1110407.150452	40.609498
3338.235637	1112646.877084	40.614516
3341.261565	1114904.147177	40.619533
3344.843858	1117148.969547	40.624551
3348.001362	1119396.626236	40.629568
3351.372083	1121661.442400	40.634586
3355.008806	1123911.395413	40.639604
3358.161877	1126163.990547	40.644621
3361.500206	1128429.830719	40.649639
3365.074373	1130692.297959	40.654656
3368.470723	1132958.949764	40.659674
3372.273602	1135222.862794	40.664692
3375.138831	1137496.664243	40.669709
3379.130392	1139745.738528	40.674727
3382.574653	1142016.180137	40.679744
3385.905300	1144280.559686	40.684762
3389.543132	1146548.644683	40.689780
3392.598432	1148817.362899	40.694797
3396.198185	1151076.326700	40.699815
3399.391536	1153350.153809	40.704832
3402.931642	1155626.149470	40.709850
3406.207541	1157888.092464	40.714868
3409.621664	1160162.897252	40.719885
3413.086606	1162422.853756	40.724903
3416.979942	1164690.525076	40.729920
3420.247359	1166970.592765	40.734938
3423.745133	1169220.828239	40.739956
3426.820050	1171483.334019	40.744973
3430.386764	1173753.428403	40.749991
3434.340169	1176021.435791	40.755008
3437.563324	1178264.256746	40.760013
3441.251824	1180434.451040	40.765018
3444.403489	1182577.944832	40.770023
3448.015143	1184632.702884	40.775028
3451.032664	1186617.341257	40.780032
3453.604430	1188527.778859	40.785037
3456.845572	1190354.421993	40.790042
3459.807103	1192113.860765	40.795047
3462.618377	1193780.504062	40.800052
3465.280622	1195374.062480	40.805056
3468.075745	1196901.502083	40.810061
3470.691872	1198335.816159	40.815066
3472.982201	1199700.182104	40.820071
3475.496890	1201000.472799	40.825076
3477.647663	1202211.987665	40.830080
3479.196695	1203370.823476	40.835085
3481.359312	1204463.414130	40.840090
3483.501907	1205501.337185	40.845095
3485.245142	1206461.923934	40.850100
3487.099866	1207375.668011	40.855104
3488.542558	1208226.011288	40.860109
3490.476030	1208995.982560	40.865114
3492.275690	1209750.506301	40.870119
3493.468633	1210438.183375	40.875124
3495.072499	1211074.222868	40.880128
3496.090810	1211666.949995	40.885133
3497.889621	1212202.680060	40.890138
3498.549756	1212704.670693	40.895143
3499.623639	1213166.782098	40.900148
3500.891837	1213579.893329	40.905152
3501.939283	1213972.147496	40.910157
3503.225214	1214327.011439	40.915162
3504.105226	1214644.786135	40.920167
3505.059381	1214920.255572	40.925172
3505.993843	1215162.420062	40.930176
3506.949335	1215383.528351	40.935181
3507.773432	1215562.567789	40.940186
3508.169819	1215730.637159	40.945191
3509.131800	1215859.802155	40.950196
3509.868294	1215976.564739	40.955200
3509.906065	1216070.531248	40.960205
3511.175145	1216123.806526	40.965210
3511.820879	1216164.748093	40.970215
3512.345567	1216185.886871	40.975220
3512.848382	1216171.124401	40.980224
3513.232770	1216164.983623	40.985229
3513.777462	1216111.316930	40.990234
3514.111343	1216070.774989	40.995239
3514.300109	1215998.464865	41.000244
3514.791394	1215916.753206	41.005248
3514.988156	1215826.111925	41.010253
3515.684704	1215718.741867	41.015258
3516.050073	1215597.116653	41.020263
3516.213459	1215458.221491	41.025268
3516.467875	1215318.185343	41.030272
3516.872136	1215166.430599	41.035277
3517.029150	1214991.050564	41.040282
3517.278644	1214822.476750	41.045287
3517.307521	1214636.069420	41.050292
3518.019052	1214429.433039	41.055296
3517.858077	1214238.459278	41.060301
3518.341282	1214019.777547	41.065306
3518.526630	1213811.612619	41.070311
3518.550579	1213579.984845	41.075316
3518.844140	1213330.246203	41.080320
3518.576042	1213103.603296	41.085325
3519.113477	1212859.040729	41.090330
3518.993922	1212601.381629	41.095335
3519.276682	1212353.936231	41.100340
3519.882871	1212087.990933	41.105344
3519.626653	1211818.804878	41.110349
3519.850643	1211542.600116	41.115354
3519.901968	1211267.531973	41.120359
3519.823282	1210978.056457	41.125364
3520.269051	1210687.167741	41.130368
3520.234629	1210405.234325	41.135373
3520.575275	1210095.607666	41.140378
3520.464423	1209801.202922	41.145383
3520.288522	1209489.190536	41.150388
3520.480357	1209172.697928	41.155392
3520.362247	1208889.945735	41.160397
3520.995395	1208566.788488	41.165402
3520.931095	1208251.592095	41.170407
3520.560598	1207926.499485	41.175412
3520.670850	1207609.923694	41.180416
3520.652384	1207292.038226	41.185421
3520.688430	1206968.784821	41.190426
3521.087881	1206650.228679	41.195431
3520.952654	1206315.533711	41.200436
3521.059129	1205989.302752	41.205440
3520.755679	1205670.614107	41.210445
3520.884947	1205327.847039	41.215450
3520.659829	1204995.516892	41.220455
3520.702753	1204656.936003	41.225460
3521.011211	1204317.539280	41.230464
3521.026647	1203994.101664	41.235469
3521.140585	1203655.255521	41.240474
3521.015104	1203310.052280	41.245479
3521.079548	1202971.262868	41.250484
3521.102806	1202619.614113	41.255488
3520.977254	1202271.247262	41.260493
3521.104229	1201931.628897	41.265498
3521.095399	1201571.006144	41.270503
3520.681313	1201231.805691	41.275508
3521.192123	1200890.461097	41.280512
3520.874039	1200546.510494	41.285517
3521.173177	1200190.148142	41.290522
3520.942504	1199862.645196	41.295527
3520.841553	1199512.023561	41.300532
3520.858660	1199153.009179	41.305536
3520.904663	1198808.131784	41.310541
3520.996302	1198456.937402	41.315546
3520.969884	1198100.390030	41.320551
3520.676296	1197747.146323	41.325556
3520.688335	1197399.740300	41.330560
3520.944998	1197045.888617	41.335565
3520.699774	1196694.629451	41.340570
3520.885294	1196360.546461	41.345575
3520.768426	1195999.362957	41.350580
3521.147573	1195638.917336	41.355584
3520.675584	1195291.918208	41.360589
3521.139910	1194936.573048	41.365594
3521.270827	1194571.023543	41.370599
3521.043155	1194218.371961	41.375604
3520.969024	1193848.391523	41.380608
3520.876816	1193503.838936	41.385613
3521.062879	1193137.521307	41.390618
3520.914731	1192762.872951	41.395623
3520.764291	1192407.079020	41.400628
3520.917677	1192047.734630	41.405632
3520.768444	1191691.421447	41.410637
3520.408246	1191334.084895	41.415642
3520.619228	1190974.186512	41.420647
3520.580046	1190617.029354	41.425652
3520.903780	1190264.298551	41.430656
3520.710760	1189906.271808	41.435661
3520.661435	1189543.215198	41.440666
3520.536953	1189192.270816	41.445671
3520.536763	1188834.608037	41.450676
3520.444469	1188473.833421	41.455680
3520.386161	1188113.592119	41.460685
3520.401627	1187757.732561	41.465690
3520.495393	1187400.049103	41.470695
3520.201430	1187050.021520	41.475700
3520.133178	1186677.363380	41.480704
3519.867853	1186326.811950	41.485709
3520.151768	1185971.913916	41.490714
3520.393719	1185629.226241	41.495719
3520.284451	1185253.274304	41.500724
3520.537438	1184898.119647	41.505728
3520.002609	1184542.976311	41.510733
3520.101632	1184180.930044	41.515738
3519.963234	1183837.339688	41.520743
3519.787101	1183475.665832	41.525748
3519.840007	1183122.963122	41.530752
3519.816199	1182783.424654	41.535757
3519.752925	1182427.117512	41.540762
3519.628987	1182075.690340	41.545767
3519.566894	1181731.665478	41.550772
3519.509374	1181376.132365	41.555776
3519.396592	1181044.778767	41.560781
3519.692259	1180675.018005	41.565786
3519.671360	1180323.549333	41.570791
3519.486700	1179979.710979	41.575796
3519.930834	1179620.585159	41.580800
3519.825596	1179275.839604	41.585805
3519.366792	1178918.414917	41.590810
3519.620697	1178578.555552	41.595815
3519.588162	1178222.143010	41.600820
3519.841489	1177861.890924	41.605824
3519.295702	1177513.238738	41.610829
3519.161800	1177163.176340	41.615834
3519.282964	1176815.686513	41.620839
3519.456156	1176475.420286	41.625844
3519.474476	1176118.195548	41.630848
3519.025980	1175782.792242	41.635853
3519.151960	1175428.989266	41.640858
3519.160048	1175084.324001	41.645863
3519.346661	1174740.737598	41.650868
3519.230191	1174379.645429	41.655872
3519.073357	1174040.122693	41.660877
3518.994144	1173692.928678	41.665882
3519.147163	1173359.344199	41.670887
3519.173570	1172999.358464	41.675892
3519.142800	1172648.786782	41.680896
3518.717524	1172321.077357	41.685901
3518.808961	1171960.066111	41.690906
3518.788497	1171617.439487	41.695911
3518.668646	1171279.145427	41.700916
3518.499762	1170934.329007	41.705920
3518.487377	1170605.311803	41.710925
3518.403986	1170265.436674	41.715930
3518.783479	1169927.350056	41.720935
3518.609859	1169605.089113	41.725940
3518.754171	1169245.107790	41.730944
3518.636855	1168912.793031	41.735949
3518.814954	1168567.385591	41.740954
3518.684609	1168236.162339	41.745959
3518.281335	1167894.109232	41.750964
3518.374251	1167550.819356	41.755968
3518.302901	1167215.934979	41.760973
3517.956935	1166869.180049	41.765978
3518.056643	1166555.842629	41.770983
3518.251369	1166216.979810	41.775988
3518.427447	1165882.158048	41.780992
3518.141802	1165543.802805	41.785997
3518.147140	1165209.532640	41.791002
3518.249575	1164876.358347	41.796007
3517.784636	1164532.867711	41.801012
3517.554142	1164205.183117	41.806016
3517.846190	1163887.687361	41.811021
3517.874356	1163563.981512	41.816026
3517.818930	1163226.571978	41.821031
3517.563165	1162893.991728	41.826036
3517.823516	1162567.918751	41.831040
3517.479138	1162249.200257	41.836045
3517.234869	1161924.398604	41.841050
3517.325323	1161599.238202	41.846055
3517.312332	1161280.311684	41.851060
3517.312873	1160952.007423	41.856064
3517.151256	1160638.736715	41.861069
3517.235204	1160316.238634	41.866074
3517.048126	1159995.088685	41.871079
3517.283279	1159683.964149	41.876084
3517.351909	1159351.956379	41.881088
3517.166804	1159036.324963	41.886093
3517.021758	1158712.347865	41.891098
3517.158663	1158397.948666	41.896103
3517.296533	1158075.871280	41.901108
3517.109542	1157759.501466	41.906112
3517.301404	1157448.535216	41.911117
3517.083346	1157119.365066	41.916122
3516.784646	1156799.834835	41.921127
3516.999220	1156480.957323	41.926132
3517.021374	1156164.078592	41.931136
3516.635572	1155862.667419	41.936141
3516.751396	1155552.074410	41.941146
3517.158335	1155234.224808	41.946151
3516.604549	1154929.854909	41.951156
3516.717226	1154608.325957	41.956160
3516.605298	1154301.576015	41.961165
3516.464662	1153979.104050	41.966170
3516.853521	1153669.017258	41.971175
3516.366201	1153378.458267	41.976180
3516.723463	1153056.699543	41.981184
3516.294268	1152746.125203	41.986189
3516.533901	1152426.903008	41.991194
3516.374277	1152123.062998	41.996199
3516.098173	1151826.892949	42.001204
3516.407614	1151516.408406	42.006208
3515.972841	1151212.655844	42.011213
3516.101333	1150899.229594	42.016218
3516.225616	1150603.303533	42.021223
3516.123423	1150309.292109	42.026228
3516.319889	1149998.547324	42.031232
3515.910029	1149696.313169	42.036237
3516.095664	1149399.362311	42.041242
3516.084450	1149092.481595	42.046247
3516.128855	1148787.373636	42.051252
3516.027413	1148485.682345	42.056256
3515.758871	1148194.422261	42.061261
3516.072749	1147882.775554	42.066266
3515.708909	1147594.245523	42.071271
3515.353379	1147288.548247	42.076276
3515.617654	1146987.279538	42.081280
3515.708907	1146702.795133	42.086285
3515.816252	1146396.875212	42.091290
3515.805395	1146111.048987	42.096295
3515.699366	1145816.313795	42.101300
3515.383045	1145508.137473	42.106304
3515.626169	1145222.884836	42.111309
3515.525126	1144933.028561	42.116314
3515.153794	1144639.503715	42.121319
3515.154551	1144342.298691	42.126324
3515.261433	1144062.599343	42.131328
3515.221186	1143774.850150	42.136333
3515.132396	1143473.628793	42.141338
3515.370651	1143198.697948	42.146343
3515.204762	1142910.258613	42.151348
3515.540180	1142618.970743	42.156352
3515.179236	1142329.014458	42.161357
3515.111820	1142037.286699	42.166362
3515.405850	1141738.369460	42.171367
3514.822944	1141458.551126	42.176372
3514.983427	1141171.575790	42.181376
3514.723550	1140886.836068	42.186381
3514.980733	1140609.395878	42.191386
3515.049496	1140329.220758	42.196391
3514.853331	1140043.476413	42.201396
3514.960421	1139754.630315	42.206400
3514.783126	1139478.246185	42.211405
3514.834465	1139173.435680	42.216410
3514.891151	1138905.998421	42.221415
3514.589612	1138621.902980	42.226420
3514.545070	1138345.248062	42.231424
3514.814840	1138073.272805	42.236429
3514.465780	1137781.356908	42.241434
3514.402176	1137507.414155	42.246439
3514.607130	1137238.444429	42.251444
3514.792430	1136952.470547	42.256448
3514.725540	1136679.909653	42.261453
3514.520308	1136397.767872	42.266458
3514.603855	1136113.189715	42.271463
3514.242160	1135845.002282	42.276468
3514.308807	1135561.821698	42.281472
3514.293436	1135296.588301	42.286477
3514.295620	1135017.187956	42.291482
3514.418864	1134731.674440	42.296487
3514.183912	1134463.491296	42.301492
3514.313138	1134197.704278	42.306496
3514.134201	1133931.669741	42.311501
3514.117285	1133654.385638	42.316506
3514.244484	1133378.583348	42.321511
3514.063348	1133107.377820	42.326516
3514.002206	1132834.618510	42.331520
3513.921949	1132576.100710	42.336525
3513.816094	1132294.864667	42.341530
3514.021303	1132032.377563	42.346535
3513.884669	1131760.810913	42.351540
3514.035874	1131487.567391	42.356544
3513.961757	1131227.272359	42.361549
3513.928372	1130963.821415	42.366554
3513.766760	1130694.770639	42.371559
3513.777501	1130440.031010	42.376564
3513.661611	1130166.478458	42.381568
3513.612286	1129908.206090	42.386573
3513.639530	1129636.313851	42.391578
3513.817998	1129378.358531	42.396583
3513.372448	1129126.673512	42.401588
3513.707577	1128854.785731	42.406592
3513.456303	1128582.885564	42.411597
3513.271419	1128338.632221	42.416602
3513.394669	1128073.395838	42.421607
3513.206566	1127817.992900	42.426612
3513.138491	1127557.707582	42.431616
3513.124155	1127300.729544	42.436621
3513.084668	1127050.781719	42.441626
3513.127653	1126808.037609	42.446631
3512.968622	1126560.274197	42.451636
3513.000926	1126295.439913	42.456640
3513.190096	1126049.402840	42.461645
3512.976082	1125802.184045	42.466650
3512.939989	1125542.841566	42.471655
3512.525334	1125298.010969	42.476660
3512.974478	1125052.265666	42.481664
3513.014249	1124799.344738	42.486669
3512.564869	1124553.153506	42.491674
3512.963253	1124310.712979	42.496679
3512.649280	1124061.526701	42.501684
3512.902943	1123813.948396	42.506688
3512.810180	1123570.793781	42.511693
3512.594498	1123327.743516	42.516698
3512.595041	1123073.414727	42.521703
3512.390804	1122826.437159	42.526708
3512.354206	1122596.650650	42.531712
3512.356376	1122355.233723	42.536717
3512.510623	1122103.879788	42.541722
3512.818208	1121860.962191	42.546727
3512.323021	1121627.591665	42.551732
3512.479784	1121384.201182	42.556736
3512.246633	1121145.053498	42.561741
3512.134090	1120896.543302	42.566746
3512.676096	1120672.673089	42.571751
3512.173134	1120429.823946	42.576756
3512.404948	1120184.271362	42.581760
3512.453729	1119948.452232	42.586765
3512.274212	1119713.422265	42.591770
3512.330391	1119466.722726	42.596775
3511.912173	1119231.234634	42.601780
3512.216598	1118991.140033	42.606784
3511.895521	1118768.761163	42.611789
3512.054097	1118532.766280	42.616794
3511.878087	1118297.006639	42.621799
3512.067914	1118071.561270	42.626804
3512.179998	1117827.825743	42.631808
3512.040198	1117596.412097	42.636813
3511.791746	1117371.295273	42.641818
3512.037200	1117134.843314	42.646823
3511.904893	1116910.069135	42.651828
3512.146431	1116664.829930	42.656832
3512.008688	1116444.039660	42.661837
3511.765314	1116215.156569	42.666842
3511.732121	1115972.694842	42.671847
3511.448361	1115748.087468	42.676852
3511.846671	1115526.027293	42.681856
3512.015449	1115297.799692	42.686861
3511.594051	1115062.891303	42.691866
3511.648747	1114836.760074	42.696871
3511.368118	1114620.494122	42.701876
3511.365525	1114391.207458	42.706880
3511.666203	1114169.869922	42.711885
3511.419940	1113947.659857	42.716890
3511.693532	1113725.164263	42.721895
3511.308661	1113505.247134	42.726900
3511.375036	1113285.628105	42.731904
3511.484408	1113054.835485	42.736909
3511.204403	1112830.105227	42.741914
3511.218798	1112621.530202	42.746919
3511.302193	1112408.834584	42.751924
3511.172792	1112179.665030	42.756928
3511.247281	1111955.602800	42.761933
3511.381550	1111734.192211	42.766938
3511.263138	1111519.777644	42.771943
3510.863334	1111297.960073	42.776948
3511.057422	1111081.759442	42.781952
3511.070136	1110877.696077	42.786957
3511.082710	1110654.543783	42.791962
3511.232678	1110440.423548	42.796967
3510.361711	1110221.024337	42.801972
3510.581232	1110016.989632	42.806977
3510.608916	1109814.123832	42.811981
3510.279596	1109607.205908	42.816986
3510.786060	1109400.524078	42.821991
3510.697325	1109206.243063	42.826996
3510.246033	1108978.707703	42.832001
3510.670652	1108771.728881	42.837005
3510.647257	1108575.600963	42.842010
3510.538880	1108366.594588	42.847015
3510.646761	1108175.680036	42.852020
3510.600641	1107966.552411	42.857025
3511.053796	1107761.152729	42.862029
3510.416906	1107547.905994	42.867034
3510.455652	1107332.534756	42.872039
3510.591132	1107139.383188	42.877044
3510.544840	1106933.461365	42.882049
3510.758697	1106725.579300	42.887053
3510.529023	1106501.148783	42.892058
3510.908434	1106310.982673	42.897063
3510.743411	1106102.757027	42.902068
3510.688551	1105887.247890	42.907073
3510.483482	1105687.033979	42.912077
3510.102045	1105487.128163	42.917082
3510.597188	1105272.076811	42.922087
3509.884058	1105080.805681	42.927092
3510.122959	1104865.398279	42.932097
3509.957549	1104674.118003	42.937101
3509.922609	1104483.382541	42.942106
3510.097701	1104283.531420	42.947111
3510.174333	1104095.151822	42.952116
3510.138514	1103884.813164	42.957121
3510.320878	1103688.664315	42.962125
3509.660255	1103499.621087	42.967130
3509.789834	1103306.906230	42.972135
3509.881397	1103107.025249	42.977140
3510.346297	1102914.241136	42.982145
3509.974506	1102721.970125	42.987149
3509.673887	1102533.406992	42.992154
3509.883728	1102339.784406	42.997159
3509.604168	1102143.846547	43.002164
3510.069116	1101951.314691	43.007169
3509.452904	1101765.643505	43.012173
3509.385470	1101580.640077	43.017178
3509.697120	1101376.358194	43.022183
3509.700103	1101196.204094	43.027188
3510.120739	1100995.903969	43.032193
3509.886844	1100820.077312	43.037197
3509.978328	1100631.765446	43.042202
3509.885551	1100424.646643	43.047207
3509.671173	1100235.606633	43.052212
3509.868336	1100049.742425	43.057217
3509.842449	1099859.033085	43.062221
3509.653627	1099655.150898	43.067226
3509.295429	1099477.293348	43.072231
3509.281664	1099293.732367	43.077236
3508.881164	1099111.280561	43.082241
3509.300752	1098941.021720	43.087245
3509.086848	1098759.770289	43.092250
3509.317112	1098569.546933	43.097255
3509.146927	1098396.308215	43.102260
3509.245308	1098216.517103	43.107265
3509.442370	1098038.329465	43.112269
3509.258808	1097854.938830	43.117274
3509.096572	1097670.964640	43.122279
3509.150061	1097491.156797	43.127284
3509.170915	1097311.730921	43.132289
3509.285195	1097128.457870	43.137293
3509.113744	1096951.251559	43.142298
3509.347292	1096768.807520	43.147303
3508.893722	1096601.679694	43.152308
3508.961491	1096423.460137	43.157313
3509.326283	1096247.577327	43.162317
3508.918779	1096063.971498	43.167322
3508.894591	1095891.298106	43.172327
3509.096628	1095729.775419	43.177332
3508.732973	1095537.629809	43.182337
3509.142526	1095368.503912	43.187341
3508.777684	1095203.997233	43.192346
3509.396841	1095021.813503	43.197351
3509.086101	1094851.546209	43.202356
3508.854117	1094676.763194	43.207361
3508.918976	1094489.868398	43.212365
3508.782329	1094311.612959	43.217370
3508.908949	1094140.389999	43.222375
3508.874747	1093975.695829	43.227380
3509.078245	1093799.855764	43.232385
3508.971788	1093624.922413	43.237389
3508.714170	1093444.169938	43.242394
3509.089213	1093265.508658	43.247399
3508.782485	1093109.447301	43.252404
3508.758570	1092927.203330	43.257409
3508.674913	1092751.089362	43.262413
3508.721776	1092581.649014	43.267418
3509.126906	1092401.231219	43.272423
3508.598615	1092245.277185	43.277428
3509.006996	1092062.550013	43.282433
3509.041930	1091895.483567	43.287437
3509.100390	1091740.854455	43.292442
3509.241373	1091548.196910	43.297447
3509.154718	1091374.336569	43.302452
3508.635325	1091193.456372	43.307457
3508.731247	1091017.064983	43.312461
3508.327378	1090859.039727	43.317466
3508.432380	1090692.116177	43.322471
3508.626610	1090519.522801	43.327476
3508.610761	1090351.555288	43.332481
3508.755635	1090183.747640	43.337485
3508.440061	1090025.396243	43.342490
3508.559342	1089849.920772	43.347495
3508.322458	1089689.439568	43.352500
3508.716176	1089516.494106	43.357505
3508.552966	1089349.381863	43.362509
3508.091304	1089189.306021	43.367514
3508.483198	1089019.122814	43.372519
3508.068391	1088862.956980	43.377524
3508.204115	1088700.181939	43.382529
3508.164818	1088544.519866	43.387533
3507.926176	1088376.240513	43.392538
3508.147432	1088213.724206	43.397543
3508.055663	1088061.026818	43.402548
3508.057526	1087905.148026	43.407553
3507.723328	1087764.554122	43.412557
3507.729822	1087604.929310	43.417562
3508.105363	1087448.400984	43.422567
3507.806893	1087296.195220	43.427572
3507.491712	1087138.238606	43.432577
3507.678226	1086993.035318	43.437581
3507.524300	1086844.242777	43.442586
3507.726945	1086697.495698	43.447591
3507.560492	1086554.926251	43.452596
3507.530137	1086398.147032	43.457601
3507.544555	1086247.777068	43.462605
3507.706187	1086104.950106	43.467610
3507.898822	1085952.434131	43.472615
3507.517380	1085811.797462	43.477620
3507.551525	1085653.452612	43.482625
3507.705398	1085512.240785	43.487629
3507.503570	1085357.856081	43.492634
3507.786025	1085207.604913	43.497639
3507.636853	1085062.405351	43.502644
3507.504583	1084909.913650	43.507649
3507.827255	1084765.778797	43.512653
3507.292336	1084621.206170	43.517658
3507.577495	1084464.894442	43.522663
3507.465422	1084326.284105	43.527668
3507.651900	1084176.883129	43.532673
3507.664833	1084031.054089	43.537677
3507.400159	1083888.814409	43.542682
3507.203821	1083738.218006	43.547687
3507.146654	1083601.785458	43.552692
3507.017647	1083453.183653	43.557697
3507.117647	1083330.142612	43.562701
3506.985186	1083185.465532	43.567706
3507.221331	1083043.888416	43.572711
3507.071256	1082903.330200	43.577716
3506.958747	1082761.131877	43.582721
3507.181121	1082626.355032	43.587725
3506.707234	1082490.059155	43.592730
3506.827591	1082353.182458	43.597735
3506.798805	1082228.699139	43.602740
3507.035569	1082084.219710	43.607745
3506.786831	1081953.819827	43.612749
3506.943232	1081819.897118	43.617754
3507.207013	1081674.059540	43.622759
3507.014370	1081547.957035	43.627764
3507.041660	1081420.280619	43.632769
3507.201480	1081283.466472	43.637773
3506.778332	1081142.907788	43.642778
3506.992792	1081007.036982	43.647783
3507.106547	1080871.659039	43.652788
3506.768791	1080726.662644	43.657793
3507.008987	1080604.784105	43.662797
3506.951883	1080480.361439	43.667802
3507.096813	1080331.437445	43.672807
3506.685036	1080205.052120	43.677812
3506.696244	1080070.342778	43.682817
3506.707148	1079942.634443	43.687821
3506.600520	1079821.946917	43.692826
3506.719799	1079682.124769	43.697831
3506.876860	1079556.686212	43.702836
3506.794689	1079423.799438	43.707841
3506.755326	1079303.569151	43.712845
3506.556265	1079165.609437	43.717850
3506.883240	1079024.104847	43.722855
3506.766857	1078910.020342	43.727860
3506.717538	1078768.571101	43.732865
3506.953170	1078633.981257	43.737869
3506.341773	1078515.363361	43.742874
3506.418405	1078385.208377	43.747879
3506.730605	1078256.931067	43.752884
3506.626668	1078135.437945	43.757889
3506.562831	1078017.294917	43.762893
3506.263828	1077892.085167	43.767898
3506.527524	1077763.708270	43.772903
3506.603877	1077643.134368	43.777908
3506.638479	1077515.173318	43.782913
3506.564421	1077384.059362	43.787917
3506.572193	1077265.024309	43.792922
3506.625593	1077125.915473	43.797927
3506.478413	1077009.108329	43.802932
3506.474049	1076880.658821	43.807937
3506.583858	1076754.203596	43.812941
3506.414905	1076637.680107	43.817946
3506.478026	1076514.587274	43.822951
3505.983001	1076393.983882	43.827956
3505.968983	1076274.930833	43.832961
3506.466702	1076158.287312	43.837965
3506.103929	1076032.565323	43.842970
3506.450371	1075910.948511	43.847975
3505.947652	1075803.968169	43.852980
3505.987874	1075678.939839	43.857985
3506.252645	1075562.994151	43.862989
3505.966808	1075454.146738	43.867994
3506.057893	1075337.744738	43.872999
3506.125861	1075215.486105	43.878004
3506.009220	1075105.067355	43.883009
3506.086805	1074983.282115	43.888013
3506.113610	1074876.292421	43.893018
3506.178192	1074752.295299	43.898023
3506.043271	1074641.774158	43.903028
3506.088305	1074510.763686	43.908033
3506.489567	1074391.120971	43.913037
3505.774146	1074284.914272	43.918042
3505.796942	1074159.469857	43.923047
3505.911692	1074057.252184	43.928052
3506.000859	1073945.719536	43.933057
3506.052801	1073816.996610	43.938061
3506.058906	1073719.785474	43.943066
3506.166957	1073590.759808	43.948071
3506.212777	1073482.106667	43.953076
3505.946441	1073362.359280	43.958081
3505.997508	1073238.233983	43.963085
3505.975286	1073138.807646	43.968090
3506.323283	1073006.654486	43.973095
3506.086065	1072907.547569	43.978100
3506.051410	1072788.037666	43.983105
3505.847330	1072674.701977	43.988109
3505.902364	1072560.264396	43.993114
3505.857345	1072447.954679	43.998119
3505.985802	1072340.994718	44.003124
3506.029898	1072214.349191	44.008129
3506.287048	1072101.117825	44.013133
3505.856750	1072000.200616	44.018138
3505.852465	1071869.999807	44.023143
3506.112283	1071771.366988	44.028148
3506.093747	1071651.637425	44.033153
3505.894048	1071533.953116	44.038157
3505.710726	1071423.182696	44.043162
3505.716720	1071308.150419	44.048167
3505.619644	1071203.415694	44.053172
3505.589446	1071102.992652	44.058177
3505.464880	1070999.027380	44.063181
3505.534382	1070894.067089	44.068186
3505.766635	1070783.888044	44.073191
3505.656972	1070686.449860	44.078196
3505.420895	1070572.210885	44.083201
3505.674936	1070471.537221	44.088205
3505.272370	1070368.182449	44.093210
3505.581354	1070253.270345	44.098215
3505.485425	1070153.994157	44.103220
3505.457348	1070052.974783	44.108225
3505.824985	1069946.986015	44.113229
3505.553483	1069849.463469	44.118234
3505.786807	1069747.145761	44.123239
3505.813691	1069636.112307	44.128244
3505.805793	1069519.891196	44.133249
3505.828314	1069414.814169	44.138253
3505.455745	1069309.511791	44.143258
3505.924715	1069201.088516	44.148263
3505.679651	1069105.374985	44.153268
3505.656509	1068991.644807	44.158273
3505.784322	1068876.829828	44.163277
3505.712106	1068776.947921	44.168282
3505.593319	1068660.630705	44.173287
3505.336018	1068559.910000	44.178292
3505.544431	1068467.860455	44.183297
3505.582454	1068345.837842	44.188301
3505.130013	1068246.105036	44.193306
3505.226128	1068139.741434	44.198311
3505.322094	1068036.549017	44.203316
3505.238994	1067940.403827	44.208321
3505.395754	1067845.179062	44.213325
3504.979347	1067750.047045	44.218330
3505.154965	1067647.507332	44.223335
3505.324225	1067555.256591	44.228340
3505.319443	1067448.703874	44.233345
3505.696405	1067333.815554	44.238349
3505.290698	1067242.423614	44.243354
3505.282937	1067145.290355	44.248359
3505.366242	1067043.620125	44.253364
3505.216435	1066954.681807	44.258369
3505.195369	1066851.871087	44.263373
3505.222320	1066755.783183	44.268378
3504.971876	1066657.430906	44.273383
3505.029040	1066553.832258	44.278388
3505.061936	1066450.043279	44.283393
3504.984571	1066366.469907	44.288397
3504.816181	1066272.329459	44.293402
3505.276983	1066172.023744	44.298407
3505.356934	1066086.881151	44.303412
3504.806438	1065991.163541	44.308417
3504.866949	1065888.706115	44.313421
3504.918229	1065803.179060	44.318426
3504.959783	1065713.419522	44.323431
3504.732592	1065609.272684	44.328436
3504.543816	1065528.687126	44.333441
3504.830282	1065440.037207	44.338445
3504.831331	1065354.415231	44.343450
3504.991826	1065266.937730	44.348455
3505.207678	1065171.464425	44.353460
3504.887436	1065084.351818	44.358465
3505.165894	1064993.771819	44.363469
3504.984860	1064895.568950	44.368474
3505.212932	1064796.623440	44.373479
3504.809034	1064713.944620	44.378484
3504.832532	1064607.716945	44.383489
3504.911155	1064512.158565	44.388493
3504.789109	1064432.508123	44.393498
3505.058316	1064343.843361	44.398503
3505.024289	1064256.093132	44.403508
3504.502238	1064162.744542	44.408513
3504.951860	1064072.506071	44.413517
3504.851092	1063981.875623	44.418522
3504.792332	1063894.316147	44.423527
3504.895165	1063802.301972	44.428532
3504.677200	1063723.426904	44.433537
3504.952514	1063620.603083	44.438541
3504.719680	1063542.016566	44.443546
3504.630310	1063449.162001	44.448551
3504.626209	1063369.380478	44.453556
3504.678617	1063292.283248	44.458561
3504.858044	1063198.032790	44.463565
3504.816613	1063112.671593	44.468570
3504.861356	1063028.546075	44.473575
3504.678784	1062933.003251	44.478580
3504.706629	1062842.429071	44.483585
3505.087903	1062757.955238	44.488589
3504.451730	1062677.594021	44.493594
3504.625034	1062574.959951	44.498599
3504.712794	1062489.760310	44.503604
3504.438118	1062409.816912	44.508609
3504.704283	1062324.777845	44.513613
3504.425675	1062239.345890	44.518618
3504.619497	1062154.027319	44.523623
3504.838134	1062066.104243	44.528628
3504.420590	1061987.429647	44.533633
3504.495053	1061889.997338	44.538637
3504.358248	1061818.975359	44.543642
3504.356937	1061728.098823	44.548647
3504.725170	1061639.181599	44.553652
3504.798398	1061554.740029	44.558657
3504.807943	1061470.307652	44.563661
3504.566102	1061394.580101	44.568666
3504.726333	1061306.847060	44.573671
3504.606868	1061234.081701	44.578676
3504.222634	1061147.783680	44.583681
3504.477882	1061053.772824	44.588685
3504.555353	1060976.638998	44.593690
3504.949506	1060895.215470	44.598695
3504.271111	1060809.827143	44.603700
3504.312023	1060735.103071	44.608705
3504.419016	1060646.597984	44.613709
3504.093346	1060573.280119	44.618714
3504.588809	1060495.011521	44.623719
3504.585072	1060407.483730	44.628724
3503.980643	1060337.578847	44.633729
3504.383518	1060264.522046	44.638733
3504.353672	1060181.231906	44.643738
3504.270963	1060098.238104	44.648743
3504.338499	1060021.766612	44.653748
3504.257794	1059943.585075	44.658753
3503.964459	1059857.251829	44.663757
3503.924507	1059794.180766	44.668762
3504.126269	1059718.742287	44.673767
3504.239116	1059643.606334	44.678772
3503.743553	1059581.763539	44.683777
3504.051755	1059491.569535	44.688781
3504.089593	1059432.622755	44.693786
3504.152395	1059360.380447	44.698791
3504.101583	1059289.889509	44.703796
3503.846799	1059214.808254	44.708801
3504.123738	1059143.202018	44.713805
3503.935638	1059064.544113	44.718810
3504.284066	1058983.388800	44.723815
3503.848167	1058892.633327	44.728820
3504.221135	1058849.517613	44.733825
3504.354483	1058762.615325	44.738829
3503.977104	1058696.023392	44.743834
3504.251565	1058617.379238	44.748839
3504.149104	1058529.645203	44.753844
3503.799084	1058473.930756	44.758849
3504.238653	1058394.003987	44.763853
3504.217337	1058321.665582	44.768858
3503.985558	1058261.113088	44.773863
3504.081792	1058176.808565	44.778868
3503.875080	1058104.112514	44.783873
3504.095356	1058017.954820	44.788877
3503.922262	1057954.499279	44.793882
3503.976309	1057874.917485	44.798887
3503.873881	1057813.953424	44.803892
3503.751436	1057745.381258	44.808897
3503.994859	1057664.705516	44.813901
3503.628585	1057603.204540	44.818906
3503.962632	1057540.238745	44.823911
3504.255776	1057479.398516	44.828916
3503.861284	1057396.222648	44.833921
3504.211151	1057325.640577	44.838925
3503.945619	1057249.185446	44.843930
3503.747324	1057175.512282	44.848935
3503.915283	1057119.891514	44.853940
3504.065605	1057051.747537	44.858945
3504.097203	1056967.916920	44.863949
3504.056892	1056905.390945	44.868954
3504.211955	1056823.850276	44.873959
3504.019382	1056746.412606	44.878964
3503.979887	1056681.667773	44.883969
3504.268704	1056601.547143	44.888973
3503.741384	1056540.735334	44.893978
3503.815159	1056477.703919	44.898983
3503.737322	1056398.122525	44.903988
3503.885935	1056341.726201	44.908993
3503.694101	1056266.112555	44.913997
3503.665676	1056197.023814	44.919002
3503.686380	1056129.371615	44.924007
3503.849732	1056066.995319	44.929012
3503.864487	1056005.413744	44.934017
3504.026265	1055932.339238	44.939021
3503.863484	1055861.437389	44.944026
3503.835357	1055789.934215	44.949031
3503.627539	1055716.628606	44.954036
3503.603729	1055657.555218	44.959041
3503.956766	1055589.359786	44.964045
3503.368575	1055542.617868	44.969050
3503.980194	1055471.487084	44.974055
3503.586387	1055407.556670	44.979060
3503.550820	1055338.169207	44.984065
3503.972444	1055270.054916	44.989069
3503.859884	1055213.979225	44.994074
3503.591722	1055135.953084	44.999079
3503.656589	1055076.280561	45.004084
3503.434976	1055011.449726	45.009089
3503.712206	1054936.126130	45.014093
3503.069692	1054884.375419	45.019098
3503.065173	1054818.639065	45.024103
3503.836333	1054759.232346	45.029108
3503.711118	1054711.539606	45.034113
3503.541826	1054645.924726	45.039117
3503.516596	1054581.152881	45.044122
3503.757722	1054528.482141	45.049127
3503.852188	1054463.207225	45.054132
3503.339591	1054404.297316	45.059137
3503.600078	1054345.837835	45.064141
3503.412410	1054292.367885	45.069146
3503.642893	1054224.754178	45.074151
3503.616494	1054153.904313	45.079156
3503.240270	1054084.267984	45.084161
3503.484930	1054021.662376	45.089165
3503.442257	1053974.817302	45.094170
3503.250308	1053907.558498	45.099175
3503.526625	1053845.716926	45.104180
3503.739519	1053789.380338	45.109185
3503.573544	1053711.220804	45.114189
3503.464633	1053667.276296	45.119194
3503.436477	1053595.166224	45.124199
3503.561015	1053540.577047	45.129204
3503.252097	1053479.502647	45.134209
3503.620881	1053429.307137	45.139213
3503.520055	1053380.634736	45.144218
3503.324715	1053309.030535	45.149223
3503.550246	1053245.647956	45.154228
3503.430735	1053193.891642	45.159233
3503.797980	1053130.002307	45.164237
3503.627281	1053079.603218	45.169242
3503.585227	1052998.134899	45.174247
3503.525590	1052938.074083	45.179252
3503.398152	1052874.456114	45.184257
3503.915613	1052806.006388	45.189261
3503.555876	1052764.699472	45.194266
3503.497879	1052689.400447	45.199271
3503.751040	1052629.284756	45.204276
3503.749735	1052573.067473	45.209281
3503.645812	1052504.234211	45.214285
3503.314137	1052441.994916	45.219290
3503.437833	1052386.719460	45.224295
3503.458291	1052317.477656	45.229300
3503.318448	1052263.498003	45.234305
3503.086097	1052210.690281	45.239309
3503.385039	1052164.930808	45.244314
3503.367738	1052100.900043	45.249319
3503.262461	1052047.201895	45.254324
3503.123632	1051987.433098	45.259329
3503.284209	1051930.893301	45.264333
3503.180765	1051875.071498	45.269338
3502.949962	1051810.108118	45.274343
3503.325929	1051766.357944	45.279348
3503.090354	1051714.510435	45.284353
3503.225048	1051654.017876	45.289357
3503.049021	1051606.788896	45.294362
3503.121751	1051558.746970	45.299367
3503.123570	1051506.954860	45.304372
3503.062390	1051443.020145	45.309377
3503.312004	1051396.780200	45.314381
3502.969088	1051341.764043	45.319386
3503.123742	1051297.467912	45.324391
3502.790189	1051247.561176	45.329396
3502.886026	1051196.232929	45.334401
3502.879745	1051151.479870	45.339405
3503.212969	1051095.964090	45.344410
3502.992693	1051041.214103	45.349415
3503.690992	1050991.135104	45.354420
3503.183424	1050935.080994	45.359425
3503.191849	1050856.273578	45.364429
3503.154755	1050816.345816	45.369434
3502.864491	1050761.025823	45.374439
3502.930577	1050710.951956	45.379444
3502.903847	1050663.497399	45.384449
3502.977323	1050600.591845	45.389453
3503.132921	1050568.926385	45.394458
3502.662644	1050530.611324	45.399463
3503.428807	1050491.513562	45.404468
3503.055462	1050428.969042	45.409473
3502.771318	1050368.627869	45.414477
3503.198048	1050323.507390	45.419482
3503.141234	1050278.466183	45.424487
3503.249298	1050217.769360	45.429492
3503.069088	1050164.451135	45.434497
3503.028511	1050115.740037	45.439501
3503.088020	1050073.668624	45.444506
3503.201793	1050015.766342	45.449511
3503.026550	1049962.445350	45.454516
3503.153759	1049911.003533	45.459521
3503.099288	1049851.294211	45.464525
3503.115256	1049803.246382	45.469530
3502.933599	1049757.353198	45.474535
3503.042299	1049710.736461	45.479540
3502.876661	1049649.403129	45.484545
3502.959627	1049606.455981	45.489549
3503.037323	1049576.727286	45.494554
3503.079428	1049514.586396	45.499559
3503.031410	1049473.878880	45.504564
3502.815936	1049430.497106	45.509569
3502.852245	1049371.250067	45.514573
3502.891859	1049329.562210	45.519578
3502.761713	1049275.937713	45.524583
3502.776689	1049223.832589	45.529588
3502.622643	1049183.526348	45.534593
3502.664763	1049134.117569	45.539597
3503.064305	1049091.596729	45.544602
3502.744899	1049048.711524	45.549607
3502.690967	1049007.808572	45.554612
3502.812378	1048962.534311	45.559617
3502.884843	1048902.793843	45.564621
3502.810854	1048871.349471	45.569626
3502.708069	1048814.531713	45.574631
3503.118197	1048774.612043	45.579636
3502.886753	1048731.227412	45.584641
3503.034891	1048676.200326	45.589645
3502.582910	1048632.079265	45.594650
3502.591538	1048593.189392	45.599655
3502.886947	1048550.488554	45.604660
3502.874892	1048517.101989	45.609665
3502.761142	1048452.369352	45.614669
3502.737055	1048404.508974	45.619674
3502.718861	1048368.323979	45.624679
3503.019943	1048321.277845	45.629684
3502.853049	1048276.238462	45.634689
3502.789619	1048231.085168	45.639693
3503.049468	1048197.458883	45.644698
3502.531178	1048137.710950	45.649703
3502.755024	1048082.762003	45.654708
3502.927691	1048047.798069	45.659713
3502.909259	1047993.660204	45.664717
3502.694473	1047959.049050	45.669722
3502.965471	1047896.755785	45.674727
3502.715622	1047869.484626	45.679732
3502.633485	1047826.840394	45.684737
3502.752929	1047766.886907	45.689741
3502.781842	1047732.909789	45.694746
3502.538054	1047687.299197	45.699751
3502.876144	1047638.793463	45.704756
3502.521989	1047609.318358	45.709761
3502.908683	1047573.833606	45.714765
3502.522882	1047528.534643	45.719770
3502.282288	1047486.589506	45.724775
3502.179408	1047447.902986	45.729780
3502.308938	1047431.859795	45.734785
3502.454602	1047378.943631	45.739789
3502.197642	1047364.411691	45.744794
3502.481822	1047324.984926	45.749799
3502.898547	1047267.872683	45.754804
3502.598601	1047226.900564	45.759809
3502.044928	1047179.888997	45.764813
3502.669738	1047131.910742	45.769818
3502.492158	1047016.400145	45.774823
3502.726493	1046860.856689	45.779828
3502.390224	1046646.325503	45.784833
3502.758751	1046360.715611	45.789837
3502.389921	1046023.176025	45.794842
3502.304576	1045622.715514	45.799847
3502.112347	1045148.087449	45.804852
3501.902498	1044619.054440	45.809857
3501.889923	1044026.583810	45.814861
3502.079439	1043355.200177	45.819866
3502.178105	1042630.812591	45.824871
3502.060582	1041832.068891	45.829876
3501.456334	1040967.291848	45.834881
3501.472867	1040024.960501	45.839885
3501.436764	1039020.129516	45.844890
3501.167602	1037949.507581	45.849895
3501.300227	1036788.776389	45.854900
3500.595667	1035561.297858	45.859905
3500.780468	1034252.521683	45.864909
3500.594081	1032877.307826	45.869914
3500.219835	1031415.249833	45.874919
3500.039189	1029883.548334	45.879924
3499.358372	1028269.282595	45.884929
3499.473961	1026560.832788	45.889933
3499.160263	1024799.115036	45.894938
3498.638547	1022954.960131	45.899943
3498.732106	1021007.204627	45.904948
3498.171118	1018996.307697	45.909953
3498.119714	1016883.676451	45.914957
3497.672974	1014694.491631	45.919962
3497.522329	1012437.972140	45.924967
3497.237445	1010085.348151	45.929972
3496.532095	1007656.669800	45.934977
3496.103831	1005132.566956	45.939981
3495.694743	1002547.398680	45.944986
3495.245202	999861.377570	45.949991
3495.050014	997102.264336	45.954996
3494.395811	994266.369418	45.960001
3494.020594	991334.448315	45.965005
3493.469768	988328.278979	45.970010
3492.526141	985235.290530	45.975015
3492.607626	982064.680524	45.980020
3492.199135	978832.205219	45.985025
3491.403241	975498.544942	45.990029
3490.875113	972085.525573	45.995034
3490.286576	968587.876257	46.000039
3490.097043	965017.319627	46.005044
3489.443475	961358.089013	46.010049
3488.837402	957615.525844	46.015053
3488.299540	953801.392830	46.020058
3487.164889	950001.390213	46.025063
3486.836371	946105.916264	46.030068
3485.561466	942144.302512	46.035073
3485.165970	938093.194861	46.040077
3484.194621	933986.636826	46.045082
3483.889693	929797.804146	46.050087
3482.988085	925487.700724	46.055092
3481.979019	921137.205386	46.060097
3481.291785	916697.641484	46.065101
3480.257889	912174.815308	46.070106
3479.313501	907577.939131	46.075111
3478.882274	902898.203300	46.080116
3478.220387	898139.233771	46.085121
3476.841490	893281.995049	46.090125
3475.921454	888364.029836	46.095130
3475.061750	883365.238644	46.100135
3474.560488	878275.132115	46.105140
3473.227120	873124.967596	46.110145
3472.315871	867878.201139	46.115149
3471.137239	862552.731114	46.120154
3470.204022	857140.535778	46.125159
3469.320151	851652.090402	46.130164
3468.088734	846089.461362	46.135169
3467.127516	840441.434309	46.140173
3466.007688	834714.653240	46.145178
3464.812905	828898.061260	46.150183
3463.667761	822999.584504	46.155188
3462.634414	817034.827458	46.160193
3461.475151	810967.316115	46.165197
3460.388785	804846.401176	46.170202
3459.167369	798631.699797	46.175207
3458.169408	792326.272841	46.180212
3456.734055	785953.624281	46.185217
3455.148611	779482.602400	46.190221
3454.488260	772945.911592	46.195226
3452.876526	766326.715863	46.200231
3451.748365	759613.695749	46.205236
3450.225851	752840.235178	46.210241
3449.102946	745966.540998	46.215245
3447.819304	739026.340532	46.220250
3446.259479	731995.018043	46.225255
3445.144866	724881.544448	46.230260
3443.464366	717680.576422	46.235265
3441.940027	710406.928456	46.240269
3440.441432	703053.098365	46.245274
3438.820523	695619.076374	46.250279
3437.351667	688098.017632	46.255284
3436.009768	680526.952229	46.260289
3434.503892	672854.275507	46.265293
3432.905588	665116.587337	46.270298
3431.514083	657286.946518	46.275303
3429.787393	649385.303608	46.280308
3427.947030	641405.190371	46.285313
3426.153478	633353.550260	46.290317
3424.762870	625223.243733	46.295322
3422.634355	617026.313670	46.300327
3421.362644	608752.166479	46.305332
3418.868882	600402.086321	46.310337
3417.535375	591971.305250	46.315341
3415.741948	583484.067365	46.320346
3413.921836	574908.098119	46.325351
3412.039698	566247.672165	46.330356
3410.049045	557547.794565	46.335361
3408.125985	548753.785124	46.340365
3406.242684	539896.068580	46.345370
3404.381943	530971.987301	46.350375
3402.294822	521958.667722	46.355380
3400.129778	512897.812210	46.360385
3398.336509	503745.972611	46.365389
3396.234353	494546.767644	46.370394
3394.139445	485279.009634	46.375399
3391.860466	475914.820331	46.380404
3389.405551	466515.321099	46.385409
3387.339469	457041.696978	46.390413
3384.886399	447499.919444	46.395418
3382.515137	437913.380230	46.400423
3380.465865	428259.667513	46.405428
3378.018866	418530.360916	46.410433
3375.529641	408737.127292	46.415437
3372.926815	398894.524405	46.420442
3370.139483	389002.725543	46.425447
3367.682858	379046.838794	46.430452
3365.077396	369047.729978	46.435457
3362.539742	359012.392499	46.440461
3359.793741	348897.534233	46.445466
3357.022531	338739.055723	46.450471
3354.260395	328539.473218	46.455476
3351.262968	318295.755810	46.460481
3348.638547	307997.785348	46.465485
3345.718159	297660.279870	46.470490
3342.334396	287277.820366	46.475495
3339.082574	276861.828195	46.480500
3336.392396	266413.725793	46.485505
3333.344808	255921.206492	46.490509
3329.791663	245386.563196	46.495514
3326.497406	234826.308170	46.500519
3323.148098	224182.446544	46.505524
3319.489644	213529.631802	46.510529
3315.557579	202890.178113	46.515533
3312.015910	192236.979267	46.520538
3308.337915	181563.948691	46.525543
3304.551739	170865.781716	46.530548
3300.399764	160175.156601	46.535553
3296.229350	149469.946312	46.540557
3291.587377	138767.675585	46.545562
3287.345411	128071.068876	46.550567
3283.351635	117357.484057	46.555572
3278.131835	106687.369643	46.560577
3273.325490	96017.682956	46.565581
3267.961454	85373.817141	46.570586
3261.703426	74760.307155	46.575591
3255.736375	64189.619144	46.580596
3248.845213	53710.186487	46.585601
3239.985448	43322.934061	46.590605
3217.313721	33405.643658	46.595610
3187.191130	23909.983301	46.600615
3156.207297	14851.640398	46.605620
3109.391632	6740.132978	46.610625
3005.619340	940.022948	46.615629
2760.980479	395.868011	46.620634
2603.776387	410.651980	46.625639
2570.757544	405.326526	46.630644
2626.795867	381.083197	46.635649
2718.746702	356.969742	46.640653
2803.655007	342.814817	46.645658
2858.683924	358.564191	46.650663
2882.935974	363.114555	46.655668
2883.218242	361.069079	46.660673
2871.757329	355.224105	46.665677
2857.781091	340.173817	46.670682
2845.846721	347.482857	46.675687
2838.654166	338.891932	46.680692
2834.609986	351.285891	46.685697
2833.379152	357.683962	46.690701
2832.581506	341.762701	46.695706
2831.714939	336.403754	46.700711
2830.212761	326.684609	46.705716
2827.617680	334.794169	46.710721
2824.470434	336.580676	46.715725
2821.182031	335.689185	46.720730
2817.663453	338.393861	46.725735
2815.478999	327.049826	46.730740
2812.068462	322.590465	46.735745
2808.884003	331.130561	46.740749
2805.844592	327.014418	46.745754
2802.369130	330.578212	46.750759
2799.550893	325.183005	46.755764
2796.562986	326.548915	46.760769
2793.113690	319.947469	46.765773
2789.765008	316.702965	46.770778
2786.418255	325.722762	46.775783
2783.174695	316.159519	46.780788
2779.880512	315.838358	46.785793
2776.767850	305.860194	46.790797
2774.000848	315.133066	46.795802
2770.094880	310.603081	46.800807
2767.520188	314.535644	46.805812
2763.972480	322.600416	46.810817
2759.896466	308.977608	46.815821
2757.081512	304.907853	46.820826
2753.340227	303.648677	46.825831
2750.187123	300.405395	46.830836
2746.591826	301.355381	46.835841
2743.476719	314.891355	46.840845
2740.775893	307.083569	46.845850
2736.757531	307.657475	46.850855
2733.329282	307.964397	46.855860
2730.083505	308.314638	46.860865
2726.262250	307.609899	46.865869
2723.282768	305.727603	46.870874
2719.876696	308.668798	46.875879
2716.510841	298.483105	46.880884
2713.349093	293.998173	46.885889
2709.315170	294.511024	46.890893
2706.096215	287.621069	46.895898
2702.461148	302.205379	46.900903
2699.683131	282.075124	46.905908
2695.960802	291.278305	46.910913
2692.256400	290.305305	46.915917
2689.184322	281.360268	46.920922
2685.222488	293.666571	46.925927
2682.296634	280.626993	46.930932
2679.291415	288.756340	46.935937
2675.804893	289.828222	46.940941
2672.463808	271.197502	46.945946
2668.493987	289.962389	46.950951
2664.845776	290.492665	46.955956
2660.892593	275.849999	46.960961
2657.535890	284.037600	46.965965
2654.586549	270.395269	46.970970
2651.238937	279.579691	46.975975
2648.134035	288.430691	46.980980
2644.271577	289.682864	46.985985
2640.370861	289.152479	46.990989
2637.397170	269.651913	46.995994
2633.609766	284.705111	47.000999
2630.826105	270.266337	47.006004
2627.161911	275.986896	47.011009
2623.273250	278.323210	47.016013
2620.186347	279.571429	47.021018
2616.550054	286.475829	47.026023
2613.511466	277.784977	47.031028
2610.204122	278.629534	47.036033
2606.204693	273.320571	47.041037
2602.663768	272.871665	47.046042
2599.142002	282.584327	47.051047
2596.173116	268.135073	47.056052
2592.333506	273.504442	47.061057
2588.441880	270.298070	47.066061
2585.339220	267.402508	47.071066
2581.915482	278.286455	47.076071
2578.234180	268.774516	47.081076
2575.204865	267.314668	47.086081
2571.784252	265.467098	47.091085
2568.351925	269.135248	47.096090
2564.670425	281.160557	47.101095
2561.346231	261.138624	47.106100
2557.448906	271.176342	47.111105
2553.926441	278.427521	47.116109
2550.751617	269.939614	47.121114
2547.005035	272.929526	47.126119
2543.402718	264.925001	47.131124
2540.566261	268.999638	47.136129
2536.897673	273.461987	47.141133
2533.707083	272.593269	47.146138
2529.651024	267.478675	47.151143
2526.446580	267.597738	47.156148
2522.546329	263.773650	47.161153
2519.478469	263.527950	47.166157
2515.933114	261.370867	47.171162
2512.409888	264.533806	47.176167
2509.036453	261.332005	47.181172
2505.708138	258.436497	47.186177
2501.536123	255.477082	47.191181
2498.574548	250.341755	47.196186
2494.805054	259.206287	47.201191
2491.586314	259.019122	47.206196
2487.774253	253.804337	47.211201
2484.352801	260.230180	47.216205
2481.312367	252.839428	47.221210
2477.949444	246.461899	47.226215
2474.436373	255.407375	47.231220
2471.010498	252.933160	47.236225
2466.806028	250.785743	47.241229
2463.136475	261.135574	47.246234
2459.786013	257.518705	47.251239
2456.880918	250.295662	47.256244
2453.290915	255.483337	47.261249
2449.699754	253.856037	47.266253
2446.171326	247.151340	47.271258
2442.630990	249.028266	47.276263
2439.358647	259.117357	47.281268
2435.708952	252.013564	47.286273
2432.202825	252.107241	47.291277
2429.089927	246.389566	47.296282
2425.476641	255.077910	47.301287
2421.823763	245.911822	47.306292
2418.358293	249.207242	47.311297
2414.564879	245.276709	47.316301
2411.301789	247.995154	47.321306
2407.494679	251.500926	47.326311
2403.999564	246.800215	47.331316
2400.906468	246.216285	47.336321
2397.170137	245.038857	47.341325
2394.169758	248.106147	47.346330
2390.610308	251.009031	47.351335
2386.977628	254.548496	47.356340
2383.405523	252.284013	47.361345
2379.982623	239.536445	47.366349
2376.566904	245.165214	47.371354
2372.504335	250.800033	47.376359
2369.219334	258.086006	47.381364
2366.072777	247.752200	47.386369
2362.576025	251.069477	47.391373
2358.809788	248.806834	47.396378
2355.267272	252.332035	47.401383
2351.717862	247.124919	47.406388
2348.475244	247.358482	47.411393
2344.870044	242.886592	47.416397
2341.769235	238.691224	47.421402
2337.845860	243.271539	47.426407
2334.116167	242.269842	47.431412
2331.188110	243.449750	47.436417
2327.362456	240.811668	47.441421
2324.245220	239.347683	47.446426
2320.645777	240.298054	47.451431
2316.857739	248.123790	47.456436
2313.055759	247.225579	47.461441
2309.703182	246.717731	47.466445
2306.752148	252.434549	47.471450
2303.236834	238.169626	47.476455
2299.783429	246.158210	47.481460
2295.938304	241.759855	47.486465
2292.271380	244.400517	47.491469
2288.839969	236.534201	47.496474
2285.496781	242.696025	47.501479
2282.041181	228.916535	47.506484
2278.653247	234.238864	47.511489
2274.954808	248.462368	47.516493
2271.698311	236.103164	47.521498
2267.686633	234.115661	47.526503
2264.256330	240.714113	47.531508
2261.321765	235.832629	47.536513
2257.562047	226.680422	47.541517
2254.055597	228.150307	47.546522
2250.534713	233.859114	47.551527
2246.883273	237.531664	47.556532
2243.776473	233.286029	47.561537
2239.969038	236.173152	47.566541
2236.810739	230.640053	47.571546
2232.851628	229.217197	47.576551
2229.644185	232.599278	47.581556
2225.808371	224.204013	47.586561
2222.458828	241.691769	47.591565
2219.444071	237.085662	47.596570
2215.686070	232.352053	47.601575
2212.078083	236.608901	47.606580
2208.457565	234.139790	47.611585
2204.947868	234.714820	47.616589
2201.483287	229.915755	47.621594
2198.148922	234.531972	47.626599
2194.679802	228.061025	47.631604
2191.222911	230.350005	47.636609
2187.317395	225.979632	47.641613
2183.907960	218.559537	47.646618
2180.636238	234.905034	47.651623
2177.221838	235.111264	47.656628
2173.743278	219.983737	47.661633
2170.131774	229.335934	47.666637
2167.000130	226.792324	47.671642
2162.874415	241.983921	47.676647
2159.472298	228.924564	47.681652
2156.168111	228.270586	47.686657
2152.217686	239.329234	47.691661
2149.262628	218.075975	47.696666
2145.399648	228.903840	47.701671
2142.018461	225.714848	47.706676
2138.853168	224.141866	47.711681
2135.133643	220.640007	47.716685
2131.494595	224.191483	47.721690
2127.863156	220.609392	47.726695
2124.825785	224.223816	47.731700
2121.114034	217.132526	47.736705
2117.738737	225.547308	47.741709
2114.231277	215.684887	47.746714
2110.801041	234.117889	47.751719
2107.134726	225.990016	47.756724
2103.412364	215.610176	47.761729
2099.845237	226.351568	47.766733
2096.602744	221.704360	47.771738
2093.117311	223.799987	47.776743
2089.720804	216.302141	47.781748
2086.147965	210.778409	47.786753
2082.620094	220.652053	47.791757
2079.226684	212.796959	47.796762
2075.582015	220.894119	47.801767
2071.971416	217.269948	47.806772
2068.842935	218.899249	47.811777
2064.869704	222.826419	47.816781
2061.472527	214.416813	47.821786
2058.290517	222.128567	47.826791
2054.788698	223.490737	47.831796
2051.161744	211.858133	47.836801
2047.736995	229.310874	47.841805
2044.623632	210.023996	47.846810
2040.432516	218.303853	47.851815
2036.937030	223.799403	47.856820
2033.401794	224.773946	47.861825
2029.825374	229.507211	47.866829
2026.385238	218.631969	47.871834
2023.109592	222.292545	47.876839
2019.373086	218.548980	47.881844
2016.600997	217.654567	47.886849
2012.710851	225.370295	47.891853
2009.241148	214.823440	47.896858
2005.357442	222.634989	47.901863
2001.614634	226.070652	47.906868
1998.739019	209.550683	47.911873
1995.228961	219.315265	47.916877
1991.669475	212.234943	47.921882
1988.058391	223.577146	47.926887
1984.648739	210.774280	47.931892
1981.012408	219.065739	47.936897
1977.190041	220.315279	47.941901
1974.511490	211.660691	47.946906
1970.691137	223.721609	47.951911
1967.105989	210.083768	47.956916
1963.664439	211.804815	47.961921
1959.831809	224.295637	47.966925
1956.601777	206.045911	47.971930
1952.960128	206.616783	47.976935
1949.715901	215.107176	47.981940
1945.943413	209.851854	47.986945
1942.552942	215.755227	47.991949
1939.455475	211.313946	47.996954
1935.915424	213.546415	48.001959
1932.130890	217.593365	48.006964
1929.133518	206.696346	48.011969
1925.213517	215.106250	48.016973
1921.429397	213.805840	48.021978
1917.649364	212.653040	48.026983
1914.356378	225.755807	48.031988
1911.419341	207.411203	48.036993
1907.713731	216.405803	48.041997
1904.111990	208.772528	48.047002
1900.407246	213.484889	48.052007
1896.703553	217.463863	48.057012
1893.790946	210.788014	48.062017
1889.942377	217.984413	48.067021
1886.545041	200.293114	48.072026
1882.903185	215.425884	48.077031
1879.753835	215.406600	48.082036
1876.565136	197.491172	48.087041
1872.517202	211.248480	48.092045
1869.106519	200.311166	48.097050
1865.601788	210.041764	48.102055
1861.913488	205.629534	48.107060
1858.537282	210.871461	48.112065
1855.015125	212.208961	48.117069
1851.490762	210.326277	48.122074
1847.649895	199.511945	48.127079
1844.343511	206.972193	48.132084
1841.206156	202.075041	48.137089
1837.616312	209.480741	48.142093
1834.110214	193.653296	48.147098
1830.668538	209.309571	48.152103
1827.099223	200.680778	48.157108
1823.636582	201.697014	48.162113
1819.690009	210.081059	48.167117
1816.306066	202.370961	48.172122
1813.363533	213.685786	48.177127
1809.969435	203.750587	48.182132
1806.491112	202.091582	48.187137
1802.373233	208.395016	48.192141
1798.788738	205.146811	48.197146
1795.592657	205.884276	48.202151
1791.753392	204.617601	48.207156
1788.595203	192.168204	48.212161
1784.832470	197.450650	48.217165
1781.812225	198.092910	48.222170
1777.804232	199.365484	48.227175
1774.106269	201.772561	48.232180
1771.238945	202.375386	48.237185
1767.589226	193.067922	48.242189
1763.811772	199.910200	48.247194
1760.876336	202.608584	48.252199
1756.683980	207.734433	48.257204
1753.478981	200.033716	48.262209
1749.925094	199.472331	48.267213
1746.860603	195.282509	48.272218
1743.006162	201.016959	48.277223
1739.482852	198.231453	48.282228
1735.957676	185.517869	48.287233
1732.159510	198.909037	48.292237
1728.595171	196.529670	48.297242
1725.282220	184.685360	48.302247
1722.185246	204.308092	48.307252
1718.937992	190.150298	48.312257
1715.099701	200.782460	48.317261
1711.436422	191.424883	48.322266
1707.979951	191.115101	48.327271
1704.031371	198.346428	48.332276
1701.124453	195.957251	48.337281
1697.714253	196.303993	48.342285
1694.157601	203.258149	48.347290
1690.752625	190.620451	48.352295
1686.652842	210.729801	48.357300
1683.326834	190.583552	48.362305
1679.482206	195.913598	48.367309
1676.684712	191.633581	48.372314
1673.353041	185.830556	48.377319
1669.799533	188.778356	48.382324
1665.799586	190.694087	48.387329
1661.876993	194.001430	48.392333
1658.793998	201.923395	48.397338
1655.651053	192.588214	48.402343
1652.049350	199.018950	48.407348
1648.924759	195.596576	48.412353
1645.059375	195.073920	48.417357
1641.339404	189.382540	48.422362
1637.750834	192.785225	48.427367
1634.199545	193.115127	48.432372
1630.808355	188.747332	48.437377
1627.396897	191.664017	48.442381
1623.811044	194.203906	48.447386
1620.264545	195.633239	48.452391
1617.030289	190.824605	48.457396
1613.601143	196.728569	48.462401
1609.715583	199.107687	48.467405
1606.397877	189.868460	48.472410
1603.053561	197.203054	48.477415
1599.177464	193.125533	48.482420
1595.981119	199.524226	48.487425
1592.003709	204.668163	48.492429
1588.982851	179.413820	48.497434
1586.067263	193.125444	48.502439
1582.376401	194.718416	48.507444
1578.543450	189.374539	48.512449
1574.690768	198.962983	48.517453
1570.926181	191.344257	48.522458
1567.661439	188.885838	48.527463
1564.177352	193.241403	48.532468
1560.966135	183.239975	48.537473
1557.465525	189.173512	48.542477
1553.953685	184.784037	48.547482
1550.512830	187.946525	48.552487
1546.800707	195.384163	48.557492
1543.382322	186.942257	48.562497
1539.770695	197.045382	48.567501
1536.535454	183.959596	48.572506
1532.920380	185.337247	48.577511
1529.097753	197.780499	48.582516
1525.926101	186.689707	48.587521
1522.257133	197.272202	48.592525
1518.926322	177.792707	48.597530
1515.251976	183.112484	48.602535
1511.334711	191.189840	48.607540
1508.659552	186.856758	48.612545
1505.101522	194.115474	48.617549
1501.397328	181.750838	48.622554
1497.607893	189.650831	48.627559
1494.226589	182.583036	48.632564
1490.979849	183.675870	48.637569
1487.257314	185.793640	48.642573
1483.577864	180.183966	48.647578
1480.128761	181.677500	48.652583
1476.730724	185.260531	48.657588
1473.734225	170.110279	48.662593
1470.112253	187.239049	48.667597
1466.244789	183.846240	48.672602
1462.898015	180.280778	48.677607
1458.812455	181.477440	48.682612
1455.551179	180.850846	48.687617
1452.389848	188.877359	48.692621
1448.988867	190.777223	48.697626
1445.686809	180.957189	48.702631
1441.647577	181.500018	48.707636
1438.753236	170.496310	48.712641
1434.995123	182.324870	48.717645
1431.217141	177.550237	48.722650
1427.711158	177.074440	48.727655
1424.012878	183.735394	48.732660
1420.652470	178.841828	48.737665
1417.085436	185.471948	48.742669
1413.849928	177.401567	48.747674
1410.178019	176.448145	48.752679
1406.294305	183.298746	48.757684
1403.212745	175.186685	48.762689
1400.027060	181.528144	48.767693
1396.391658	178.827030	48.772698
1392.704130	176.290695	48.777703
1388.746967	189.120737	48.782708
1385.922601	181.912046	48.787713
1382.226312	187.535028	48.792717
1378.410202	170.695173	48.797722
1375.199946	181.370016	48.802727
1371.521682	182.573495	48.807732
1368.575634	177.618273	48.812737
1365.175942	181.239608	48.817741
1361.584498	181.114861	48.822746
1357.879342	178.973612	48.827751
1353.937561	182.539602	48.832756
1350.536219	183.841518	48.837761
1346.751734	183.177522	48.842765
1343.675225	183.091997	48.847770
1340.377849	177.031329	48.852775
1336.640149	177.737840	48.857780
1333.577128	179.628441	48.862785
1329.577928	186.299449	48.867789
1326.129954	176.391993	48.872794
1322.773237	175.793844	48.877799
1318.864919	182.254023	48.882804
1315.525771	177.874652	48.887809
1312.104620	185.401199	48.892813
1308.940682	183.051563	48.897818
1305.178863	180.938736	48.902823
1301.421232	177.270108	48.907828
1298.415034	179.501079	48.912833
1294.240131	181.167782	48.917837
1290.976553	178.945985	48.922842
1287.614774	179.683207	48.927847
1283.980406	179.049615	48.932852
1280.598035	173.416774	48.937857
1277.231074	176.663279	48.942861
1273.721770	179.790626	48.947866
1270.325251	169.799046	48.952871
1266.557984	175.553563	48.957876
1263.416338	170.113429	48.962881
1259.715304	183.707063	48.967885
1256.373205	180.794039	48.972890
1252.873478	176.549040	48.977895
1248.585007	177.339906	48.982900
1245.591872	174.802383	48.987905
1242.244759	187.692593	48.992909
1238.658357	182.030904	48.997914
1235.171280	178.787452	49.002919
1231.312947	179.050447	49.007924
1228.248642	182.785577	49.012929
1224.318160	177.231111	49.017933
1221.224019	171.692886	49.022938
1217.571811	171.065531	49.027943
1213.633465	179.392057	49.032948
1210.979349	167.731726	49.037953
1207.065250	178.418537	49.042957
1203.512121	164.703342	49.047962
1200.374988	177.117015	49.052967
1196.456994	179.567015	49.057972
1193.162581	170.497433	49.062977
1189.643471	175.597679	49.067981
1186.115996	176.174462	49.072986
1182.554999	167.928277	49.077991
1178.803801	175.705684	49.082996
1175.488349	161.501897	49.088001
1172.063204	170.986384	49.093005
1168.000929	181.168487	49.098010
1165.117949	172.946425	49.103015
1161.248121	181.242033	49.108020
1158.202943	168.190228	49.113025
1154.568332	167.229604	49.118029
1150.987660	178.481052	49.123034
1147.830012	170.502446	49.128039
1144.117364	173.998360	49.133044
1140.642831	171.676801	49.138049
1136.956423	171.126069	49.143053
1133.340644	183.481460	49.148058
1130.268299	175.303206	49.153063
1126.353797	172.694196	49.158068
1122.999820	166.122488	49.163073
1119.444011	168.415560	49.168077
1115.644755	174.016990	49.173082
1112.517260	163.456543	49.178087
1109.223831	163.206073	49.183092
1105.592749	163.718019	49.188097
1101.977989	172.674364	49.193101
1098.232579	172.790638	49.198106
1095.337075	165.223981	49.203111
1091.396727	161.992108	49.208116
1087.870480	162.839449	49.213121
1084.397278	166.835605	49.218125
1080.755415	177.207705	49.223130
1077.502549	164.969519	49.228135
1073.589654	172.216661	49.233140
1070.592406	163.455917	49.238145
1067.446446	163.170465	49.243149
1063.213769	168.674974	49.248154
1059.970951	160.036074	49.253159
1056.256793	164.324780	49.258164
1052.750643	167.944791	49.263169
1049.526253	170.679911	49.268173
1045.813516	169.283658	49.273178
1042.454577	165.371583	49.278183
1039.016683	162.969842	49.283188
1035.395428	161.130623	49.288193
1032.405547	160.920146	49.293197
1028.257343	166.266296	49.298202
1025.044438	168.595338	49.303207
1021.310096	169.188799	49.308212
1018.013166	160.955353	49.313217
1014.384645	161.206672	49.318221
1010.699542	156.280918	49.323226
1007.475274	162.878988	49.328231
1003.842845	157.315908	49.333236
1000.493012	147.080025	49.338241
996.720449	165.200522	49.343245
993.276105	157.670971	49.348250
989.930336	157.338142	49.353255
986.363878	161.699376	49.358260
982.986498	157.604612	49.363265
979.352446	166.274540	49.368269
975.636937	164.787923	49.373274
972.901563	161.203165	49.378279
968.908150	158.396555	49.383284
965.297982	153.179558	49.388289
961.610844	152.560084	49.393293
957.926185	153.768090	49.398298
954.606107	158.842680	49.403303
951.273435	166.053664	49.408308
947.977783	158.501264	49.413313
944.592225	166.056116	49.418317
941.132140	158.835914	49.423322
937.564881	158.903130	49.428327
933.461587	170.283575	49.433332
930.470817	160.678926	49.438337
926.779715	168.611379	49.443341
923.521191	153.392569	49.448346
919.910489	164.048446	49.453351
916.093095	171.516966	49.458356
912.868210	154.892490	49.463361
909.246256	163.719186	49.468365
905.856635	159.023109	49.473370
902.413926	150.811045	49.478375
898.190067	160.720925	49.483380
895.204641	157.503548	49.488385
891.850080	162.851019	49.493389
888.060695	158.768698	49.498394
885.152882	152.148715	49.503399
881.106484	160.712548	49.508404
877.968741	161.099743	49.513409
874.455284	164.814276	49.518413
870.508640	154.445769	49.523418
867.254823	163.479346	49.528423
863.628416	162.871405	49.533428
860.252664	158.733918	49.538433
856.723552	164.530106	49.543437
853.149104	155.896762	49.548442
850.020424	155.434729	49.553447
846.057858	158.773766	49.558452
842.506132	156.365377	49.563457
839.495196	150.815296	49.568461
835.548148	162.648657	49.573466
832.319610	155.397980	49.578471
828.796346	155.588905	49.583476
825.411282	146.651528	49.588481
821.623034	154.333006	49.593485
818.028554	152.554404	49.598490
814.654474	159.254242	49.603495
810.983053	155.562993	49.608500
807.951153	147.414655	49.613505
804.472476	162.384477	49.618509
800.616538	161.115107	49.623514
797.636791	151.634996	49.628519
793.431727	161.191996	49.633524
789.859844	155.116695	49.638529
786.561968	149.801274	49.643533
782.993940	160.259953	49.648538
779.852219	159.441890	49.653543
775.852453	161.149236	49.658548
773.095443	149.023024	49.663553
769.401209	157.763358	49.668557
765.874327	153.136989	49.673562
762.198117	153.587316	49.678567
758.295418	151.107107	49.683572
754.999710	154.643080	49.688577
751.595700	161.151072	49.693581
748.226494	158.700064	49.698586
744.898070	152.521741	49.703591
741.030784	153.003734	49.708596
737.254089	151.388948	49.713601
734.315686	149.937704	49.718605
730.807521	148.686020	49.723610
727.323941	153.800931	49.728615
723.048201	156.588481	49.733620
720.086091	148.230466	49.738625
716.791467	153.137583	49.743629
713.181252	155.328068	49.748634
710.263021	140.138252	49.753639
706.098490	163.684306	49.758644
702.345370	154.296159	49.763649
698.831445	152.468509	49.768653
695.481222	151.684034	49.773658
692.252955	150.975904	49.778663
688.651046	151.458198	49.783668
685.283505	149.280225	49.788673
681.529324	160.956315	49.793677
677.842726	160.079914	49.798682
674.708554	147.945510	49.803687
670.847679	159.677010	49.808692
667.669259	147.526242	49.813697
663.833684	141.380431	49.818701
660.360791	155.589108	49.823706
657.083191	142.338745	49.828711
653.516258	152.390440	49.833716
650.179631	143.394760	49.838721
646.780410	151.983328	49.843725
642.835204	164.199653	49.848730
639.666517	153.480847	49.853735
635.940864	147.963678	49.858740
632.598472	148.050152	49.863745
628.915957	147.683251	49.868749
625.554971	155.928213	49.873754
622.458386	155.659285	49.878759
618.251718	155.063364	49.883764
614.825984	146.839400	49.888769
611.601919	148.436282	49.893773
607.850780	146.983980	49.898778
604.908578	143.991053	49.903783
601.166159	153.770069	49.908788
597.520155	147.699338	49.913793
593.875166	157.853928	49.918797
590.334491	157.343162	49.923802
587.231296	155.200700	49.928807
583.337772	150.661536	49.933812
579.960098	136.109826	49.938817
576.276142	156.612260	49.943821
572.973779	147.988516	49.948826
569.684366	141.332483	49.953831
565.655806	161.050812	49.958836
562.782069	155.169617	49.963841
558.770537	141.309217	49.968845
555.447451	152.878240	49.973850
552.492039	162.096661	49.978855
548.428149	145.005084	49.983860
544.789311	145.786955	49.988865
541.430665	156.626981	49.993869
537.655202	150.854198	49.998874
534.430279	148.694382	50.003879
531.111387	146.591721	50.008884
527.693011	138.958529	50.013889
524.007704	147.300905	50.018893
520.033444	154.817230	50.023898
517.171400	145.511200	50.028903
513.251228	155.338562	50.033908
509.746925	147.262108	50.038913
506.421967	144.802148	50.043917
503.234813	146.263451	50.048922
500.087672	145.233819	50.053927
496.049295	147.143735	50.058932
492.380812	146.080852	50.063937
488.942895	139.869469	50.068941
485.021680	156.248782	50.073946
481.843615	146.137662	50.078951
478.258887	147.047960	50.083956
475.000248	154.998465	50.088961
471.461294	150.252722	50.093965
467.457027	158.080356	50.098970
464.431144	139.428128	50.103975
460.920789	150.671781	50.108980
457.488380	132.250388	50.113985
453.869432	141.688048	50.118989
450.239516	143.974660	50.123994
447.069459	138.565611	50.128999
443.120376	142.977785	50.134004
439.380750	147.054662	50.139009
435.914546	142.338557	50.144013
432.588170	159.878960	50.149018
429.200560	146.076985	50.154023
425.845833	155.479502	50.159028
422.300960	146.478602	50.164033
419.239566	147.571905	50.169037
415.596612	151.638844	50.174042
411.792429	151.220246	50.179047
408.058473	151.896758	50.184052
404.563429	148.558708	50.189057
401.131286	145.854683	50.194061
397.681755	139.151704	50.199066
394.791735	147.096392	50.204071
390.960738	148.577986	50.209076
387.505458	151.693783	50.214081
383.865689	155.792078	50.219085
380.142172	153.424073	50.224090
376.636662	140.841160	50.229095
373.208437	151.145999	50.234100
369.671208	149.023755	50.239105
366.416203	148.468386	50.244109
362.625313	144.930134	50.249114
359.440037	148.192432	50.254119
355.480118	153.623875	50.259124
351.959987	142.006361	50.264129
348.717790	141.775630	50.269133
345.044127	153.769550	50.274138
341.852612	140.543450	50.279143
338.342546	149.661395	50.284148
334.839423	147.726406	50.289153
331.504451	141.818243	50.294157
327.755298	143.800934	50.299162
324.349682	146.146647	50.304167
320.655591	149.671591	50.309172
316.898536	140.117935	50.314177
313.927103	139.395089	50.319181
310.272224	149.034782	50.324186
306.911805	138.038189	50.329191
303.113423	146.229962	50.334196
299.796830	144.798687	50.339201
296.252354	152.253792	50.344205
292.289220	143.292091	50.349210
289.222342	139.528904	50.354215
285.937336	147.334183	50.359220
282.515407	138.813442	50.364225
279.059950	143.885345	50.369229
275.072158	145.181001	50.374234
271.540463	138.365791	50.379239
267.784920	150.244330	50.384244
264.226402	143.624451	50.389249
260.781763	151.594134	50.394253
257.819696	145.193083	50.399258
254.929902	139.686435	50.404263
250.967928	141.299651	50.409268
247.251245	138.048136	50.414273
243.483581	136.593851	50.419277
240.099014	150.717158	50.424282
236.593215	137.132553	50.429287
233.181263	149.247243	50.434292
229.828581	145.303613	50.439297
226.158211	139.973601	50.444301
221.994963	147.389901	50.449306
219.147425	129.518731	50.454311
215.758383	149.545478	50.459316
211.955992	147.808384	50.464321
208.482505	148.568646	50.469325
205.028587	153.240191	50.474330
201.531603	140.513532	50.479335
197.792313	144.487685	50.484340
194.688624	141.272934	50.489345
191.615843	135.968509	50.494349
187.474583	147.510871	50.499354
184.239352	135.179497	50.504359
180.737904	130.341416	50.509364
177.153420	143.073402	50.514369
173.604250	140.502197	50.519373
169.864078	150.735843	50.524378
166.669583	139.600640	50.529383
163.110472	137.378644	50.534388
159.623629	142.271900	50.539393
156.283994	138.823278	50.544397
152.688328	143.988258	50.549402
149.217219	135.763505	50.554407
145.476701	142.526158	50.559412
141.820267	140.420982	50.564417
138.642079	137.374248	50.569421
134.953459	140.575096	50.574426
131.641772	137.911796	50.579431
127.990178	139.160275	50.584436
124.522259	140.783876	50.589441
121.355479	139.499699	50.594445
117.577294	135.939577	50.599450
113.860210	133.681464	50.604455
110.128164	145.094980	50.609460
106.739116	145.670081	50.614465
103.418743	132.200055	50.619469
100.038892	142.556697	50.624474
97.218173	128.249308	50.629479
92.784820	132.628054	50.634484
89.245807	140.996383	50.639489
86.130399	133.088962	50.644493
82.237926	141.199516	50.649498
79.219212	138.936018	50.654503
75.532451	132.784753	50.659508
72.335741	137.919361	50.664513
68.909125	131.135357	50.669517
64.753616	142.211330	50.674522
61.488018	145.029777	50.679527
57.745299	140.281458	50.684532
54.313358	137.691051	50.689537
50.960007	137.036081	50.694541
47.383381	143.254260	50.699546
43.975274	139.092894	50.704551
40.429727	148.818629	50.709556
36.636069	141.515109	50.714561
33.898663	134.813255	50.719565
29.887362	146.156152	50.724570
26.038570	141.673597	50.729575
22.656259	136.491448	50.734580
19.257033	141.530312	50.739585
16.422887	129.929598	50.744589
12.364605	143.525933	50.749594
9.188330	141.556157	50.754599
5.533853	140.911416	50.759604
2.223668	151.931388	50.764609