Thu Jun 16 10:58:16 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.613646	118.671068	0.000000
-0.016567	109.733971	0.005005
0.452237	102.601956	0.010010
0.204103	90.621193	0.015014
0.277925	97.288378	0.020019
-0.030003	85.710833	0.025024
-0.169662	81.447315	0.030029
-0.342129	66.922705	0.035034
-0.811804	59.263509	0.040038
-0.833419	45.816743	0.045043
-1.181075	39.746533	0.050048
-1.504505	30.552895	0.055053
-1.633731	7.763596	0.060058
-2.052080	13.496638	0.065062
-2.437991	12.938317	0.070067
-2.694424	0.904835	0.075072
-3.689019	5.649986	0.080077
-4.047458	-5.022480	0.085082
-4.568207	3.632921	0.090086
-4.144079	-0.751663	0.095091
-4.236573	0.925058	0.100096
-4.462682	6.276109	0.105101
-4.349884	6.977061	0.110106
-4.933521	7.935262	0.115110
-5.417392	9.971439	0.120115
-5.699105	6.985006	0.125120
-6.192698	3.605925	0.130125
-6.075492	1.623861	0.135130
-6.169050	3.634305	0.140134
-6.353047	8.828740	0.145139
-6.975817	1.766965	0.150144
-7.418216	7.818092	0.155149
-7.528327	3.248918	0.160154
-7.688746	9.500474	0.165158
-7.789212	10.145711	0.170163
-7.710748	4.816324	0.175168
-8.485490	20.140261	0.180173
-8.680230	4.516150	0.185178
-9.059376	8.923222	0.190182
-9.127832	14.320437	0.195187
-9.156676	8.631038	0.200192
-9.272266	10.765481	0.205197
-9.655680	9.968796	0.210202
-10.153020	9.566216	0.215206
-10.882729	7.365603	0.220211
-10.731737	13.033068	0.225216
-11.304810	10.811107	0.230221
-10.852187	6.881339	0.235226
-11.162623	8.090649	0.240230
-11.423280	5.836988	0.245235
-12.078752	2.938565	0.250240
-12.291551	17.881763	0.255245
-12.481263	2.801293	0.260250
-12.708475	3.764816	0.265254
-12.688263	5.620910	0.270259
-12.558876	-4.589874	0.275264
-13.480138	9.539008	0.280269
-13.914140	4.172375	0.285274
-14.096670	6.037803	0.290278
-13.963266	-2.106758	0.295283
-13.788929	2.245939	0.300288
-14.679285	5.696106	0.305293
-14.908191	6.191898	0.310298
-15.311675	9.919127	0.315302
-15.399734	4.086208	0.320307
-15.028611	4.018084	0.325312
-15.811083	5.199547	0.330317
-16.156740	-8.011407	0.335322
-16.784907	5.311969	0.340326
-17.338524	1.624456	0.345331
-16.726423	-2.670736	0.350336
-17.390828	13.274233	0.355341
-17.367464	-3.238179	0.360346
-17.146804	1.598748	0.365350
-17.427045	1.688383	0.370355
-18.323321	-4.090680	0.375360
-18.663116	8.203739	0.380365
-18.534982	14.434938	0.385370
-19.026566	-7.120772	0.390374
-18.669812	-1.898898	0.395379
-19.408673	-6.326477	0.400384
-19.969435	3.382643	0.405389
-20.328342	1.787650	0.410394
-20.020651	-0.047035	0.415398
-20.273342	-1.077525	0.420403
-20.147071	-4.817314	0.425408
-21.020808	3.883695	0.430413
-21.518194	3.602073	0.435418
-21.857333	6.757625	0.440422
-21.888423	9.752667	0.445427
-21.846332	5.479655	0.450432
-22.103021	8.910341	0.455437
-22.093933	10.670311	0.460442
-21.970782	3.981297	0.465446
-22.725623	-0.037091	0.470451
-23.464184	8.378571	0.475456
-23.665106	8.543985	0.480461
-23.675840	3.082840	0.485466
-23.567274	4.739357	0.490470
-24.156972	3.627728	0.495475
-24.423736	-4.371974	0.500480
-24.851706	4.668923	0.505485
-25.048088	-3.160001	0.510490
-25.286772	6.736017	0.515494
-25.121280	1.126280	0.520499
-25.007026	3.598707	0.525504
-26.232757	4.584296	0.530509
-26.322430	5.363201	0.535514
-27.028300	10.319508	0.540518
-26.758559	-4.226020	0.545523
-26.494121	2.216950	0.550528
-26.705115	3.098378	0.555533
-27.381098	0.188746	0.560538
-28.103895	4.576053	0.565542
-28.252564	-1.350037	0.570547
-28.179569	-5.760941	0.575552
-28.533190	13.440811	0.580557
-28.056293	1.124746	0.585562
-28.383924	7.969120	0.590566
-29.197406	4.904437	0.595571
-29.442938	5.197876	0.600576
-29.807055	3.852549	0.605581
-29.776533	6.392975	0.610586
-30.062892	-3.403125	0.615590
-30.484056	-5.290989	0.620595
-30.769237	-3.919030	0.625600
-31.475497	-2.501062	0.630605
-31.434397	6.555940	0.635610
-31.773199	6.352782	0.640614
-31.823407	16.092467	0.645619
-31.580017	5.327544	0.650624
-31.693988	10.147954	0.655629
-32.291510	2.228659	0.660634
-32.858985	1.068569	0.665638
-33.250743	1.002807	0.670643
-33.466182	3.356878	0.675648
-33.658417	13.241869	0.680653
-33.473927	-4.695085	0.685658
-33.332171	3.584071	0.690662
-34.095130	10.023596	0.695667
-34.132241	8.553888	0.700672
-34.936853	10.639323	0.705677
-35.006571	-0.584087	0.710682
-35.224056	0.556195	0.715686
-35.227447	6.034104	0.720691
-35.787406	-6.818341	0.725696
-36.337628	7.307229	0.730701
-36.289097	-4.170120	0.735706
-36.588710	0.858147	0.740710
-36.721325	1.316125	0.745715
-36.396430	-2.807103	0.750720
-37.027277	9.573297	0.755725
-37.547829	3.853289	0.760730
-37.810896	0.995777	0.765734
-38.332792	6.748592	0.770739
-38.624415	-9.118847	0.775744
-38.496545	8.521552	0.780749
-38.545125	0.927660	0.785754
-38.309175	3.339921	0.790758
-39.149410	1.073131	0.795763
-39.414388	3.353408	0.800768
-39.884854	10.169101	0.805773
-40.061843	-8.630420	0.810778
-40.011173	-4.643715	0.815782
-40.156368	-2.867425	0.820787
-40.673595	-2.099449	0.825792
-41.028435	-0.037539	0.830797
-41.043073	-9.334366	0.835802
-41.000078	1.163446	0.840806
-41.410723	-1.752940	0.845811
-42.065037	-8.306457	0.850816
-42.657336	0.856894	0.855821
-42.590813	-0.153543	0.860826
-42.739228	-2.127127	0.865830
-42.959345	0.617891	0.870835
-42.907297	-0.204192	0.875840
-42.877982	8.319661	0.880845
-43.411733	-5.194541	0.885850
-43.956792	4.184948	0.890854
-44.113016	5.410701	0.895859
-44.519262	-11.674017	0.900864
-45.371898	7.453728	0.905869
-45.534972	-10.037676	0.910874
-45.165784	-0.718322	0.915878
-45.519407	9.904726	0.920883
-45.810999	4.401801	0.925888
-46.334222	-2.825481	0.930893
-46.104967	2.679583	0.935898
-45.829968	-4.047937	0.940902
-46.324390	8.397323	0.945907
-46.826170	-2.859548	0.950912
-47.599255	10.061105	0.955917
-47.567221	-1.044950	0.960922
-47.767544	5.930309	0.965926
-47.657851	6.335912	0.970931
-47.937061	-5.930955	0.975936
-48.986265	10.014660	0.980941
-49.095454	1.052597	0.985946
-48.903097	2.027777	0.990950
-49.409150	5.409504	0.995955
-49.063327	4.553077	1.000960
-49.293011	3.260609	1.005965
-49.773708	1.640761	1.010970
-50.299617	10.331744	1.015974
-50.849946	2.948134	1.020979
-50.619958	7.173544	1.025984
-51.089655	12.872256	1.030989
-50.879089	0.801560	1.035994
-51.303184	2.633512	1.040998
-52.303009	10.298983	1.046003
-52.114633	-4.282618	1.051008
-52.623895	-0.340307	1.056013
-52.524780	-6.932509	1.061018
-52.384281	-1.410806	1.066022
-52.828635	-0.851094	1.071027
-52.737878	-10.127652	1.076032
-53.470355	8.771388	1.081037
-53.846141	4.561419	1.086042
-54.011931	2.550161	1.091046
-53.962466	0.521777	1.096051
-54.340588	-9.737915	1.101056
-55.051350	-0.071191	1.106061
-55.232572	-1.399388	1.111066
-55.433345	0.037348	1.116070
-55.747254	8.550345	1.121075
-55.318077	1.600628	1.126080
-56.026753	9.711743	1.131085
-56.040459	-1.475342	1.136090
-56.992561	3.305607	1.141094
-57.605104	0.057769	1.146099
-57.001302	-0.995785	1.151104
-57.118112	0.480052	1.156109
-57.156600	-10.245771	1.161114
-57.471542	3.035110	1.166118
-57.697003	2.555540	1.171123
-58.095128	1.193441	1.176128
-59.000292	2.014876	1.181133
-59.059163	-5.003148	1.186138
-58.683725	-0.243401	1.191142
-59.189955	1.692788	1.196147
-58.967021	-4.193592	1.201152
-60.062541	8.494844	1.206157
-60.161742	-4.239003	1.211162
-60.527614	8.205137	1.216166
-60.729110	4.672822	1.221171
-60.655548	-4.133872	1.226176
-60.899108	9.067048	1.231181
-60.610515	6.964911	1.236186
-61.367209	6.335774	1.241190
-62.143346	14.709607	1.246195
-62.087560	13.652111	1.251200
-62.547858	11.550619	1.256205
-62.489866	6.830448	1.261210
-62.753779	5.154648	1.266214
-62.700253	8.479906	1.271219
-63.384563	-3.014442	1.276224
-63.932310	3.978771	1.281229
-63.947237	10.629799	1.286234
-64.077183	4.518995	1.291238
-64.160894	7.005787	1.296243
-63.701519	2.545727	1.301248
-64.519892	2.674084	1.306253
-65.204939	0.298388	1.311258
-65.422893	6.044577	1.316262
-65.487341	-3.709170	1.321267
-65.692314	3.150346	1.326272
-65.658595	4.194262	1.331277
-66.413111	-0.659964	1.336282
-66.373690	-0.901851	1.341286
-66.798030	9.672408	1.346291
-67.290964	6.846572	1.351296
-67.158941	6.010187	1.356301
-67.098092	10.066440	1.361306
-67.686780	5.576954	1.366310
-68.400338	13.811208	1.371315
-68.257808	5.365923	1.376320
-68.449761	10.725633	1.381325
-68.869992	-4.099685	1.386330
-68.624602	2.968339	1.391334
-69.157446	5.949917	1.396339
-69.736510	-12.790048	1.401344
-70.417397	-1.932585	1.406349
-70.321927	-0.460262	1.411354
-70.419839	5.324293	1.416358
-70.557258	11.183846	1.421363
-70.092719	6.545059	1.426368
-70.680597	6.919050	1.431373
-71.198587	4.988887	1.436378
-71.574495	-1.213264	1.441382
-71.657723	-7.126980	1.446387
-71.663236	4.763545	1.451392
-72.577184	-3.053921	1.456397
-73.296617	-8.586856	1.461402
-72.602394	0.974539	1.466406
-73.106657	4.149786	1.471411
-73.180500	-1.274683	1.476416
-73.773053	1.723175	1.481421
-73.823464	-2.439937	1.486426
-73.620977	7.599810	1.491430
-74.067716	-0.289742	1.496435
-74.491648	4.580017	1.501440
-75.277025	6.584143	1.506445
-75.343391	9.332460	1.511450
-75.237474	-1.830491	1.516454
-75.504645	-2.056139	1.521459
-75.262234	-6.474914	1.526464
-75.723578	0.098751	1.531469
-76.823375	-8.703535	1.536474
-76.504159	-8.332265	1.541478
-76.951383	-4.286755	1.546483
-76.499458	-2.946544	1.551488
-77.061429	-9.183052	1.556493
-77.789135	-6.626923	1.561498
-77.937116	-2.657899	1.566502
-78.395765	4.636872	1.571507
-78.428251	-4.623857	1.576512
-78.676332	9.071469	1.581517
-78.874537	-0.373091	1.586522
-79.020345	-10.245680	1.591526
-78.812694	5.388035	1.596531
-79.234215	0.548230	1.601536
-80.041719	-3.848363	1.606541
-80.386734	5.189872	1.611546
-80.158117	-5.511334	1.616550
-80.782206	-1.688554	1.621555
-80.231004	-4.367213	1.626560
-81.016927	0.103040	1.631565
-81.678325	-1.238434	1.636570
-81.600967	-7.179182	1.641574
-82.252435	-3.741262	1.646579
-81.699175	-4.431510	1.651584
-81.809555	-6.600397	1.656589
-82.610689	-3.687043	1.661594
-82.965711	-2.814958	1.666598
-83.640054	-8.826511	1.671603
-83.405059	-9.058695	1.676608
-83.590108	4.408186	1.681613
-83.645915	1.394389	1.686618
-83.638371	-1.065186	1.691622
-84.226671	-8.611206	1.696627
-84.638518	-9.226103	1.701632
-84.914964	-10.081598	1.706637
-85.248846	-11.182423	1.711642
-85.136183	-12.437351	1.716646
-85.245886	-5.078022	1.721651
-85.592952	-9.219332	1.726656
-86.413239	2.920777	1.731661
-86.831248	-1.776165	1.736666
-86.547976	0.920384	1.741670
-86.976114	1.022331	1.746675
-86.425883	-6.289815	1.751680
-86.918201	11.774093	1.756685
-87.971485	13.167440	1.761690
-88.102048	-7.962538	1.766694
-88.496434	7.496223	1.771699
-88.337158	-9.403945	1.776704
-88.578367	3.171709	1.781709
-88.356079	1.403915	1.786714
-88.525893	1.704574	1.791718
-89.379710	8.728248	1.796723
-89.564088	7.441909	1.801728
-89.888780	13.527943	1.806733
-90.014344	10.079661	1.811738
-89.750062	-6.088296	1.816742
-90.850098	5.110431	1.821747
-91.348531	-2.063722	1.826752
-91.685458	7.860761	1.831757
-91.890554	7.282232	1.836762
-91.977952	-0.606033	1.841766
-91.850148	-0.513197	1.846771
-91.691528	-1.400148	1.851776
-91.784247	-1.547884	1.856781
-92.124074	7.018721	1.861786
-92.561279	-4.054564	1.866790
-92.830393	7.337229	1.871795
-92.848331	-1.904891	1.876800
-93.915826	9.246928	1.881805
-94.263717	8.301232	1.886810
-94.410042	1.471686	1.891814
-94.868188	5.835484	1.896819
-94.799233	-1.446747	1.901824
-94.633455	8.873913	1.906829
-94.815215	13.540083	1.911834
-94.748964	-0.513367	1.916838
-95.586566	7.242003	1.921843
-95.894484	10.305780	1.926848
-96.421295	2.358927	1.931853
-96.327635	3.995511	1.936858
-96.386939	-2.664427	1.941862
-96.624332	7.341470	1.946867
-96.273835	2.455266	1.951872
-97.492087	-0.875660	1.956877
-97.588483	0.078083	1.961882
-97.853405	-6.377693	1.966886
-97.964974	5.098552	1.971891
-98.377460	-2.487378	1.976896
-99.038994	5.429885	1.981901
-99.416794	2.829685	1.986906
-99.468310	0.352939	1.991910
-99.371296	3.297999	1.996915
-99.506631	4.185033	2.006912
-99.224033	-4.688146	2.016909
-98.386001	-2.173500	2.026906
-98.257304	-7.983721	2.036902
-98.182451	-0.703266	2.046899
-97.522375	-1.242071	2.056896
-96.346948	-3.901352	2.066893
-96.663841	-4.462176	2.076890
-95.694516	2.062660	2.086886
-95.223794	-0.260519	2.096883
-94.953564	-2.226465	2.106880
-94.142654	-6.594990	2.116877
-93.686509	6.453708	2.126874
-93.645678	-0.009251	2.136870
-93.114820	-7.019778	2.146867
-92.348383	-8.646684	2.156864
-91.230320	-3.395055	2.166861
-91.037323	-3.237614	2.176858
-90.611112	-5.955122	2.186854
-90.684820	2.691413	2.196851
-90.023272	-3.234037	2.206848
-89.529140	2.207686	2.216845
-88.669219	-2.124736	2.226842
-87.619138	1.820411	2.236838
-87.840357	0.149297	2.246835
-87.647582	5.769636	2.256832
-86.717422	7.217155	2.266829
-86.509927	8.622159	2.276826
-85.925220	-1.525673	2.286822
-85.073671	-4.508418	2.296819
-84.690262	-9.249562	2.306816
-84.647047	-6.037006	2.316813
-83.412769	-9.387540	2.326810
-83.053541	-2.612421	2.336806
-83.046956	-2.475684	2.346803
-82.194338	-0.494782	2.356800
-81.667094	-2.616455	2.366797
-81.231211	-3.788426	2.376794
-80.766291	4.660732	2.386790
-79.711599	0.413224	2.396787
-79.733946	-3.788005	2.406784
-79.757536	-1.784879	2.416781
-78.844647	-3.392525	2.426778
-78.427094	-0.309102	2.436774
-77.503781	-0.734004	2.446771
-76.694437	1.074717	2.456768
-76.663677	-6.609467	2.466765
-76.774847	3.892316	2.476762
-76.038159	2.635516	2.486758
-75.499735	-0.071546	2.496755
-74.293220	-0.309193	2.506752
-73.647076	0.714630	2.516749
-73.874357	1.638471	2.526746
-73.580988	4.035995	2.536742
-72.817977	-2.510656	2.546739
-72.108662	-6.121789	2.556736
-71.960496	-1.227962	2.566733
-71.282182	-3.957648	2.576730
-70.658033	3.678761	2.586726
-70.301209	5.174017	2.596723
-69.247576	-5.534293	2.606720
-69.044294	-5.717414	2.616717
-68.700011	-1.220791	2.626714
-68.699841	1.113519	2.636710
-67.639439	-2.709881	2.646707
-67.398757	3.185989	2.656704
-66.936289	-7.321741	2.666701
-66.154547	-5.070814	2.676698
-65.920758	1.828215	2.686694
-65.103839	1.526938	2.696691
-64.367003	-3.239427	2.706688
-64.196303	-1.266335	2.716685
-63.855442	2.028608	2.726682
-63.248112	-3.225663	2.736678
-62.784528	2.361528	2.746675
-62.225796	-0.641672	2.756672
-61.344391	-4.825274	2.766669
-61.168104	-2.828065	2.776666
-61.023544	-0.459436	2.786662
-59.756433	-6.718774	2.796659
-59.525605	4.358730	2.806656
-59.611686	-2.841685	2.816653
-59.032852	-1.550798	2.826650
-58.216820	-7.342297	2.836646
-57.557369	0.822133	2.846643
-56.556840	1.863353	2.856640
-56.755876	0.935148	2.866637
-56.361086	0.172892	2.876634
-55.897373	-3.691323	2.886630
-54.852427	-3.504776	2.896627
-54.710968	-4.593021	2.906624
-54.476989	-1.639923	2.916621
-53.120328	3.277132	2.926618
-53.113668	3.460530	2.936614
-53.088609	-3.263614	2.946611
-52.572989	4.358286	2.956608
-51.775592	-3.564862	2.966605
-51.050654	-1.741991	2.976602
-50.245531	6.812257	2.986598
-49.909663	-1.816015	2.996595
-49.778106	0.739284	3.006592
-49.686709	5.396289	3.016589
-48.483760	-5.331314	3.026586
-48.243737	-1.757989	3.036582
-47.570980	-7.131876	3.046579
-46.772582	-1.169831	3.056576
-46.604946	5.152495	3.066573
-46.531171	6.417650	3.076570
-45.704229	2.595100	3.086566
-45.201068	3.836807	3.096563
-44.597950	-1.338139	3.106560
-43.927505	3.054109	3.116557
-43.499502	11.085662	3.126554
-43.314800	3.720474	3.136550
-43.155606	0.427498	3.146547
-42.408777	4.835819	3.156544
-41.087994	6.147669	3.166541
-41.235185	0.116579	3.176538
-40.746062	5.518490	3.186534
-40.452025	0.586602	3.196531
-39.286350	-0.150535	3.206528
-39.148089	-1.818138	3.216525
-39.062009	3.700116	3.226522
-38.076781	6.957126	3.236518
-37.563932	1.396201	3.246515
-37.236913	5.891977	3.256512
-36.530385	3.044824	3.266509
-36.050243	-2.900283	3.276506
-35.919905	3.439320	3.286502
-34.604320	6.140774	3.296499
-34.295770	2.448741	3.306496
-34.241108	4.344108	3.316493
-33.989595	6.066628	3.326490
-33.231839	3.745357	3.336486
-32.867217	6.190724	3.346483
-31.592998	3.082717	3.356480
-31.436335	4.762088	3.366477
-31.061056	0.991659	3.376474
-30.804020	2.998394	3.386470
-30.248405	7.598489	3.396467
-29.325380	10.402800	3.406464
-29.465186	3.411583	3.416461
-28.451228	4.046134	3.426458
-27.800146	2.973239	3.436454
-27.543535	3.390777	3.446451
-27.478244	-1.369857	3.456448
-26.516449	2.911718	3.466445
-26.068211	-4.921771	3.476442
-25.915832	0.053202	3.486438
-24.834725	0.160978	3.496435
-23.995695	3.156727	3.506432
-24.311924	1.704796	3.516429
-24.227878	-6.815231	3.526426
-23.215751	-4.480675	3.536422
-22.641238	1.621748	3.546419
-21.404671	2.363929	3.556416
-21.322709	-2.355899	3.566413
-20.955199	2.156302	3.576410
-20.832714	10.805491	3.586406
-20.483620	2.076991	3.596403
-19.584637	-0.238872	3.606400
-19.516150	7.614976	3.616397
-18.245576	8.418856	3.626394
-17.767497	0.073840	3.636390
-17.442732	-1.084209	3.646387
-17.264433	3.375397	3.656384
-16.784609	5.038949	3.666381
-16.417555	1.930568	3.676378
-15.634923	8.786073	3.686374
-14.880941	6.701116	3.696371
-14.930226	5.834050	3.706368
-13.507212	1.634389	3.716365
-13.343135	5.873400	3.726362
-13.206471	-0.227963	3.736358
-12.719113	9.410661	3.746355
-11.960334	6.480986	3.756352
-11.252657	2.049712	3.766349
-11.274674	5.496937	3.776346
-10.792045	3.095587	3.786342
-10.151106	1.640116	3.796339
-9.671517	-3.676066	3.806336
-8.769219	-4.523127	3.816333
-8.229487	2.794356	3.826330
-8.164809	4.418055	3.836326
-8.083940	0.242041	3.846323
-6.984502	4.928491	3.856320
-6.790329	2.165516	3.866317
-5.711116	0.040495	3.876314
-5.024835	7.411404	3.886310
-5.346806	-0.605270	3.896307
-4.816929	1.004375	3.906304
-3.967076	14.650354	3.916301
-3.564727	13.187145	3.926298
-3.574080	15.057928	3.936294
-2.844560	26.420111	3.946291
-2.269980	31.562594	3.956288
-1.843387	44.610746	3.966285
-1.683074	50.727855	3.976282
-1.244552	75.966636	3.986278
-0.563234	95.045893	3.996275
-0.263652	121.525721	4.006272
0.000000	133.402957	4.011277
0.625414	134.933135	4.016282
0.453572	152.403928	4.021286
0.753155	154.914022	4.026291
1.094641	170.854917	4.031296
1.278427	181.702702	4.036301
1.458698	181.244074	4.041306
1.236438	182.032664	4.046310
1.404720	187.426629	4.051315
1.283818	186.245009	4.056320
0.977059	177.054842	4.061325
1.141934	177.374479	4.066330
0.995209	194.530309	4.071334
1.361476	183.480559	4.076339
1.293827	185.409499	4.081344
1.156190	187.995601	4.086349
1.576304	187.951641	4.091354
1.154432	190.217917	4.096358
1.684482	192.799044	4.101363
1.652413	195.830984	4.106368
1.640680	184.203037	4.111373
1.199350	167.655456	4.116378
0.977883	167.243388	4.121382
1.156944	180.451768	4.126387
1.337721	189.781368	4.131392
1.437652	193.989852	4.136397
1.348005	187.192282	4.141402
1.122791	191.497708	4.146406
1.177279	192.915658	4.151411
1.211493	186.352643	4.156416
0.800200	191.142531	4.161421
1.400850	186.220159	4.166426
1.350279	206.091167	4.171430
1.393345	208.504953	4.176435
1.602605	209.379785	4.181440
1.373303	216.680953	4.186445
1.952981	212.993349	4.191450
1.402015	213.196090	4.196454
1.815602	218.406282	4.201459
1.399903	212.117678	4.206464
1.853716	212.509531	4.211469
1.928473	213.922062	4.216474
1.439135	213.341757	4.221478
1.529032	198.212025	4.226483
1.522588	214.391789	4.231488
1.346295	221.335553	4.236493
2.011019	218.803841	4.241498
1.820676	221.606524	4.246502
1.931153	222.311421	4.251507
1.716066	214.790021	4.256512
1.367313	214.533453	4.261517
1.765800	205.361091	4.266522
1.705293	221.096379	4.271526
1.923582	216.927078	4.276531
1.900871	213.137075	4.281536
1.939686	222.631429	4.286541
2.246227	222.758364	4.291546
1.595631	202.802472	4.296550
1.674154	198.827537	4.301555
1.648038	208.032504	4.306560
1.525037	204.434781	4.311565
1.619875	208.683769	4.316570
2.093613	221.105846	4.321574
1.940462	214.094714	4.326579
1.955700	218.371460	4.331584
1.525681	216.829433	4.336589
1.847535	227.496389	4.341594
1.964579	224.006876	4.346598
1.907731	210.530470	4.351603
1.824795	223.468461	4.356608
1.861773	222.633171	4.361613
2.267784	226.208229	4.366618
1.782240	228.674252	4.371622
1.924970	216.012206	4.376627
1.734240	226.597931	4.381632
1.831146	223.237828	4.386637
2.147852	221.235987	4.391642
1.896942	223.693620	4.396646
1.781429	221.064335	4.401651
1.828489	242.372934	4.406656
1.864957	243.428943	4.411661
2.095069	242.776112	4.416666
2.131407	259.701098	4.421670
2.487439	254.088194	4.426675
2.346545	261.766630	4.431680
1.944341	252.781509	4.436685
2.122475	247.565792	4.441690
2.293836	265.726323	4.446694
2.154944	256.458842	4.451699
2.262199	251.970480	4.456704
1.994834	263.049443	4.461709
2.176736	262.839252	4.466714
2.091813	266.474535	4.471718
2.293552	260.995548	4.476723
2.341277	257.949395	4.481728
1.882174	259.533023	4.486733
2.169214	266.337988	4.491738
2.322121	264.162841	4.496742
2.266103	263.980821	4.501747
2.046248	266.722093	4.506752
2.096526	258.208249	4.511757
2.013274	259.790933	4.516762
2.002836	272.427334	4.521766
2.597574	283.025457	4.526771
2.947328	287.404495	4.531776
2.430246	273.524032	4.536781
2.423130	262.097013	4.541786
2.357921	265.125958	4.546790
2.730403	261.934782	4.551795
2.502695	265.059048	4.556800
2.457745	263.300860	4.561805
2.648798	261.699699	4.566810
2.314158	274.440781	4.571814
2.359696	257.115549	4.576819
2.140702	265.429408	4.581824
2.311220	286.146552	4.586829
2.773099	275.439054	4.591834
2.607147	296.137626	4.596838
2.909178	293.505327	4.601843
2.879573	288.644851	4.606848
2.677167	276.301622	4.611853
2.843598	262.113076	4.616858
2.647230	260.770092	4.621862
2.700603	265.958733	4.626867
2.671928	259.849435	4.631872
2.373984	266.885045	4.636877
2.529553	273.790861	4.641882
2.406223	280.124891	4.646886
2.701772	281.875141	4.651891
2.412201	295.413720	4.656896
2.558443	292.623075	4.661901
3.099341	284.210258	4.666906
2.564124	294.769890	4.671910
2.992673	288.827221	4.676915
2.863681	289.027611	4.681920
2.571342	299.243153	4.686925
2.810889	294.531561	4.691930
2.708357	290.782156	4.696934
2.990748	282.725290	4.701939
2.931040	303.485436	4.706944
2.716534	293.003550	4.711949
3.061815	282.571426	4.716954
2.970262	287.934670	4.721958
2.837435	292.985882	4.726963
2.721871	297.628968	4.731968
2.896627	288.737405	4.736973
2.782171	292.340677	4.741978
2.880427	301.327441	4.746982
2.801941	289.611396	4.751987
2.980685	290.989287	4.756992
3.034900	289.464109	4.761997
3.020331	285.810071	4.767002
2.971976	294.008239	4.772006
2.854990	288.969727	4.777011
2.886993	299.510506	4.782016
3.086868	288.061494	4.787021
2.967983	286.062570	4.792026
2.913660	300.582570	4.797030
2.947322	287.980615	4.802035
2.804783	283.278697	4.807040
2.804175	294.614893	4.812045
3.241963	313.054744	4.817050
3.392025	327.667175	4.822054
3.198840	314.303576	4.827059
2.711932	310.676880	4.832064
2.933503	318.809441	4.837069
3.585656	316.941275	4.842074
3.319871	329.780926	4.847078
3.439432	315.123867	4.852083
3.236050	311.135211	4.857088
3.078592	311.607464	4.862093
3.631446	307.950612	4.867098
3.012787	311.559766	4.872102
3.404713	305.297678	4.877107
3.215611	302.699678	4.882112
3.132883	320.918838	4.887117
3.457752	323.024537	4.892122
3.333634	314.878561	4.897126
3.478102	320.055619	4.902131
3.586227	312.330013	4.907136
3.206556	296.865501	4.912141
3.178597	295.909232	4.917146
3.672028	312.721350	4.922150
3.499006	303.352538	4.927155
3.357942	301.053616	4.932160
2.798670	299.442570	4.937165
3.562594	311.971557	4.942170
3.302055	334.774347	4.947174
3.538672	327.306300	4.952179
3.209901	319.797618	4.957184
3.592800	331.210456	4.962189
3.690540	318.112009	4.967194
3.656772	323.397446	4.972198
3.316378	324.703282	4.977203
3.337566	324.282877	4.982208
3.605381	327.757675	4.987213
3.683356	326.853845	4.992218
3.477752	333.107475	4.997222
3.248092	335.990175	5.002227
3.710376	324.354326	5.007232
3.192275	325.447922	5.012237
3.761707	327.537969	5.017242
3.729781	336.429262	5.022246
3.646738	331.297619	5.027251
3.377436	328.516445	5.032256
3.278180	334.996082	5.037261
3.481895	330.363801	5.042266
3.709544	335.365125	5.047270
3.867979	334.411693	5.052275
3.822535	333.720243	5.057280
3.405535	334.833043	5.062285
3.544379	333.017738	5.067290
3.458792	346.453791	5.072294
3.751039	354.968920	5.077299
3.807650	359.567983	5.082304
3.664733	358.957456	5.087309
3.868265	357.961647	5.092314
3.820155	362.268435	5.097318
4.089167	365.368942	5.102323
4.087887	351.975767	5.107328
3.555051	360.360778	5.112333
3.888634	357.901032	5.117338
3.925958	361.497686	5.122342
3.877506	345.854971	5.127347
3.916404	358.740682	5.132352
3.862722	359.497180	5.137357
3.937776	354.063760	5.142362
3.759116	343.801048	5.147366
3.760651	358.766478	5.152371
3.984594	350.672176	5.157376
3.996380	350.905240	5.162381
4.128079	350.001805	5.167386
3.812191	349.039347	5.172390
3.983445	357.927857	5.177395
4.212495	346.894352	5.182400
3.816092	356.298914	5.187405
4.092531	352.305539	5.192410
4.022689	350.839233	5.197414
4.000824	363.837493	5.202419
4.188453	356.392819	5.207424
3.694076	353.683661	5.212429
4.216626	353.724587	5.217434
3.673214	352.387447	5.222438
3.773587	359.606677	5.227443
3.954800	375.795062	5.232448
4.105596	378.900111	5.237453
4.354125	391.287524	5.242458
4.500090	393.237719	5.247462
4.743680	372.328212	5.252467
4.582707	367.409017	5.257472
3.988675	359.927773	5.262477
4.198662	361.146309	5.267482
4.035236	363.942498	5.272486
4.269528	359.359711	5.277491
3.978760	358.876318	5.282496
4.041731	378.308019	5.287501
4.612814	379.659361	5.292506
4.492223	389.359221	5.297510
4.359206	385.420774	5.302515
4.167013	384.787115	5.307520
4.295783	384.642431	5.312525
4.626610	380.443636	5.317530
4.424031	401.782267	5.322534
4.481847	385.205239	5.327539
4.424547	378.010280	5.332544
4.350300	376.501587	5.337549
4.383314	369.837964	5.342554
4.143937	379.765808	5.347558
4.585225	382.993330	5.352563
4.483780	390.070121	5.357568
4.338697	395.458527	5.362573
4.549072	393.849720	5.367578
4.627655	401.620900	5.372582
4.552935	393.153290	5.377587
4.585647	395.423298	5.382592
4.340334	402.989822	5.387597
4.483368	397.385724	5.392602
4.444025	397.364912	5.397606
4.591966	399.359176	5.402611
4.671210	410.447757	5.407616
4.408009	405.137006	5.412621
4.567836	391.359940	5.417626
4.354778	400.111416	5.422630
4.181475	387.807979	5.427635
4.484379	392.011289	5.432640
4.180435	395.978468	5.437645
4.621284	401.790655	5.442650
4.629540	423.523530	5.447654
4.914569	417.870209	5.452659
4.856767	422.309237	5.457664
4.446761	417.619810	5.462669
4.768950	418.511804	5.467674
4.816184	431.243677	5.472678
4.712798	425.588343	5.477683
4.942942	424.732958	5.482688
4.681955	434.297507	5.487693
4.862519	430.841254	5.492698
4.608868	436.008571	5.497702
4.853600	421.045313	5.502707
4.740700	432.523784	5.507712
4.524052	427.842454	5.512717
5.048622	432.343884	5.517722
4.643070	432.740035	5.522726
4.698623	440.702192	5.527731
4.780466	445.932852	5.532736
4.837627	438.824906	5.537741
5.053323	436.352368	5.542746
4.934208	437.578238	5.547750
4.794707	426.032882	5.552755
4.889444	428.359337	5.557760
4.949505	442.125284	5.562765
5.121985	428.048646	5.567770
4.490243	435.163369	5.572774
4.674977	437.062274	5.577779
4.990025	442.538821	5.582784
4.964599	462.050546	5.587789
5.159058	457.372796	5.592794
5.239924	467.922387	5.597798
5.256900	457.093638	5.602803
4.979935	449.286280	5.607808
4.775401	456.475933	5.612813
5.197441	456.404723	5.617818
4.799739	472.252521	5.622822
5.212851	463.960170	5.627827
4.937942	464.233806	5.632832
4.867579	469.473546	5.637837
5.142226	471.875347	5.642842
4.960103	463.978415	5.647846
5.355222	457.200456	5.652851
5.408550	461.498106	5.657856
5.348547	468.792232	5.662861
5.500505	460.383216	5.667866
5.324554	473.520191	5.672870
5.116382	471.028114	5.677875
5.435605	461.702364	5.682880
5.104166	464.787183	5.687885
5.459954	468.028557	5.692890
5.257454	463.338071	5.697894
5.456925	466.099366	5.702899
5.562266	457.477559	5.707904
5.083485	467.273656	5.712909
5.475751	459.381547	5.717914
5.676290	463.883852	5.722918
5.395508	465.858013	5.727923
5.444619	450.476983	5.732928
5.487403	460.835156	5.737933
5.413279	454.822377	5.742938
5.297776	467.205982	5.747942
5.099035	468.975587	5.752947
5.586057	458.405084	5.757952
5.467844	468.018078	5.762957
5.341768	461.398464	5.767962
5.088044	470.192907	5.772966
5.586854	460.794170	5.777971
5.527169	466.806696	5.782976
5.447350	475.178468	5.787981
5.292440	465.709979	5.792986
5.238389	474.220938	5.797990
5.241809	481.531917	5.802995
5.637741	494.314345	5.808000
5.298832	492.244810	5.813005
5.705459	501.135843	5.818010
5.704317	502.886510	5.823014
5.719515	494.110481	5.828019
5.793026	491.336654	5.833024
5.540573	495.005594	5.838029
6.030481	488.220935	5.843034
5.849829	505.601243	5.848038
5.691867	499.476021	5.853043
5.854461	502.139828	5.858048
5.585225	501.972025	5.863053
5.738232	494.213162	5.868058
6.069642	510.562343	5.873062
5.928836	503.872533	5.878067
5.994995	505.361294	5.883072
5.450186	488.859866	5.888077
6.067249	490.278304	5.893082
5.855897	499.478539	5.898086
5.892646	496.112829	5.903091
5.885059	500.110774	5.908096
5.577715	500.590044	5.913101
5.922920	497.317497	5.918106
5.870322	502.027684	5.923110
5.918886	499.151231	5.928115
6.058097	493.903880	5.933120
5.888020	496.860029	5.938125
5.854599	490.585385	5.943130
6.076638	505.850937	5.948134
5.791649	503.162791	5.953139
5.883319	503.100499	5.958144
5.391140	509.847782	5.963149
6.025830	494.632464	5.968154
5.879229	500.080154	5.973158
5.896716	497.911864	5.978163
6.177095	497.387652	5.983168
5.837412	502.727454	5.988173
6.103382	496.367716	5.993178
6.078059	495.895305	5.998182
5.918789	501.347457	6.003187
6.210118	496.706763	6.008192
6.158691	509.396600	6.013197
6.293020	497.953627	6.018202
6.202690	493.145643	6.023206
6.057343	497.973561	6.028211
6.345235	496.621562	6.033216
6.135999	500.376593	6.038221
6.379136	501.267055	6.043226
6.024237	498.155684	6.048230
6.222532	503.178489	6.053235
6.202221	496.550458	6.058240
5.854622	496.931409	6.063245
6.358109	508.754891	6.068250
5.927549	496.661004	6.073254
5.969017	503.895758	6.078259
6.158021	494.531130	6.083264
5.885554	495.419684	6.088269
6.468324	485.149041	6.093274
6.285371	501.217888	6.098278
6.082013	494.787232	6.103283
6.727833	498.375507	6.108288
6.192254	500.670483	6.113293
6.113210	506.429716	6.118298
6.150910	498.103984	6.123302
6.108682	501.654031	6.128307
6.611922	495.940550	6.133312
6.381330	485.516340	6.138317
6.303772	474.950236	6.143322
6.116228	482.622582	6.148326
5.416795	478.588293	6.153331
5.853447	487.725931	6.158336
5.660156	494.670358	6.163341
5.850670	502.366858	6.168346
6.099894	500.110352	6.173350
5.674732	498.551016	6.178355
6.394460	496.981544	6.183360
5.984364	510.175002	6.188365
5.875968	496.117390	6.193370
6.066090	500.890858	6.198374
5.414539	502.030591	6.203379
5.862634	501.985856	6.208384
5.703299	534.723518	6.213389
5.874200	534.714823	6.218394
6.011185	539.079076	6.223398
5.877629	538.514251	6.228403
6.052591	531.713349	6.233408
6.128315	536.461042	6.238413
6.376873	533.135596	6.243418
6.288277	542.013484	6.248422
6.408641	541.493713	6.253427
6.273996	538.262077	6.258432
6.219108	540.684900	6.263437
6.115097	532.456659	6.268442
6.304089	538.942417	6.273446
6.264510	540.077606	6.278451
6.416664	524.496071	6.283456
5.919888	515.977284	6.288461
5.889700	505.284253	6.293466
6.223541	520.509541	6.298470
5.937077	511.101635	6.303475
6.459034	521.966980	6.308480
5.847842	512.330873	6.313485
6.024850	528.177183	6.318490
6.112509	529.553969	6.323494
6.099574	536.057606	6.328499
6.348573	530.306412	6.333504
5.994458	522.647715	6.338509
6.307907	519.674902	6.343514
6.027588	510.391176	6.348518
5.538305	526.983237	6.353523
5.947090	528.926718	6.358528
6.372396	533.827666	6.363533
6.529968	532.106618	6.368538
6.545336	535.547709	6.373542
6.106453	517.833616	6.378547
5.993051	508.642373	6.383552
5.983962	516.835848	6.388557
6.072454	513.432084	6.393562
6.049689	511.321253	6.398566
6.241765	515.852299	6.403571
6.197662	505.772844	6.408576
5.723285	514.811349	6.413581
6.487179	527.725378	6.418586
6.284955	520.697156	6.423590
6.073022	505.190705	6.428595
6.093596	501.544423	6.433600
5.781904	512.129418	6.438605
6.137110	519.930319	6.443610
6.279838	534.303140	6.448614
6.293097	525.908426	6.453619
6.335161	517.687525	6.458624
6.338784	497.984316	6.463629
5.930774	500.340885	6.468634
5.829564	509.618820	6.473638
5.798904	512.114587	6.478643
5.907638	519.141018	6.483648
6.096113	542.400490	6.488653
6.002146	533.828742	6.493658
6.340939	543.630661	6.498662
6.294076	539.970752	6.503667
5.999244	537.964170	6.508672
6.005919	537.465258	6.513677
5.877434	537.052809	6.518682
6.070837	532.697128	6.523686
6.051665	537.935930	6.528691
6.460690	535.840854	6.533696
6.168279	541.200383	6.538701
6.143880	544.284102	6.543706
6.344180	536.673576	6.548710
6.036649	543.992463	6.553715
6.244920	536.460630	6.558720
5.937348	532.646788	6.563725
5.862101	537.290090	6.568730
6.135667	533.174512	6.573734
5.903343	538.329362	6.578739
6.169538	527.951675	6.583744
6.180194	545.089385	6.588749
6.447857	528.170505	6.593754
6.347498	538.717734	6.598758
5.945130	532.524563	6.603763
5.783703	524.294568	6.608768
5.812796	544.841473	6.613773
5.938135	538.383412	6.618778
6.117760	531.554412	6.623782
5.966348	537.574922	6.628787
6.324211	526.798214	6.633792
6.197784	539.101600	6.638797
6.055560	540.636146	6.643802
6.272659	540.517609	6.648806
6.244868	533.068493	6.653811
6.482317	526.105533	6.658816
5.910789	535.053950	6.663821
6.252539	526.941568	6.668826
6.002615	541.650392	6.673830
6.197667	545.190736	6.678835
6.238476	538.232051	6.683840
5.970482	542.577989	6.688845
6.258727	538.772036	6.693850
6.436906	543.568899	6.698854
5.993633	539.703290	6.703859
6.339054	540.102214	6.708864
5.930686	535.324477	6.713869
6.251868	534.548753	6.718874
6.072112	534.258627	6.723878
5.918071	539.943252	6.728883
6.331957	531.282253	6.733888
6.411880	532.706095	6.738893
6.281028	528.843515	6.743898
6.193280	513.727044	6.748902
5.807446	506.473157	6.753907
6.175022	500.329753	6.758912
5.701894	509.876032	6.763917
6.151338	517.382357	6.768922
6.336815	538.148276	6.773926
5.817476	523.837322	6.778931
6.390651	531.141678	6.783936
6.190078	529.287829	6.788941
6.044071	515.605194	6.793946
6.157240	511.914306	6.798950
5.913686	528.327938	6.803955
6.135518	527.274142	6.808960
6.030062	534.188976	6.813965
5.766266	539.052859	6.818970
5.977464	540.677479	6.823974
6.172226	538.739652	6.828979
6.304184	546.402836	6.833984
6.209252	541.850230	6.838989
6.241055	548.696514	6.843994
6.208391	550.870208	6.848998
6.006081	548.289739	6.854003
6.074025	543.396488	6.859008
6.024723	547.909521	6.864013
6.171451	543.748209	6.869018
6.169918	548.328525	6.874022
5.906646	547.760768	6.879027
6.130009	545.027281	6.884032
6.161654	542.836815	6.889037
6.040648	538.130076	6.894042
6.084488	547.047940	6.899046
5.922091	549.563313	6.904051
6.159402	542.487702	6.909056
6.192383	544.190510	6.914061
5.837365	539.981394	6.919066
6.245976	542.829589	6.924070
6.085820	547.065858	6.929075
5.989711	538.060076	6.934080
5.910133	543.668368	6.939085
6.233303	545.155899	6.944090
6.299868	546.350204	6.949094
5.871617	549.949158	6.954099
5.765627	548.239599	6.959104
6.131247	551.616696	6.964109
6.216796	545.795034	6.969114
6.200285	542.045263	6.974118
5.888787	544.341001	6.979123
6.122567	537.977785	6.984128
6.149730	545.937387	6.989133
6.141046	545.361990	6.994138
6.321370	538.433425	6.999142
5.923134	550.608101	7.004147
6.068646	546.049007	7.009152
6.115170	540.826428	7.014157
6.099719	542.826304	7.019162
6.334241	538.218960	7.024166
5.934327	552.777169	7.029171
6.325103	535.470340	7.034176
6.363708	540.967054	7.039181
6.244562	544.477238	7.044186
6.500757	540.454405	7.049190
6.490095	545.593147	7.054195
6.490470	537.847942	7.059200
5.997122	524.615254	7.064205
6.066601	520.754298	7.069210
6.090579	521.544832	7.074214
6.008990	542.674934	7.079219
6.309641	536.542575	7.084224
5.999726	540.278243	7.089229
6.040760	536.015419	7.094234
6.335527	530.643989	7.099238
5.956372	535.817873	7.104243
6.334196	534.617542	7.109248
5.900570	522.213175	7.114253
6.122114	531.031221	7.119258
6.448431	534.948741	7.124262
5.890655	531.696562	7.129267
6.021954	523.404578	7.134272
6.112847	526.438165	7.139277
6.239204	535.549761	7.144282
6.240549	533.851275	7.149286
6.157093	528.863574	7.154291
6.254579	508.795102	7.159296
6.287364	512.073190	7.164301
5.924977	513.272773	7.169306
6.542308	501.330491	7.174310
5.892645	516.560354	7.179315
5.751075	510.228101	7.184320
5.992212	510.150284	7.189325
5.914846	538.953694	7.194330
5.968484	529.508614	7.199334
6.196272	537.981222	7.204339
6.318459	534.060547	7.209344
6.400962	543.409364	7.214349
6.167006	526.249293	7.219354
6.123665	512.615597	7.224358
5.797785	525.347940	7.229363
6.128593	527.096634	7.234368
6.310074	534.407020	7.239373
6.251420	534.858907	7.244378
5.954456	511.775846	7.249382
5.822492	516.156025	7.254387
5.986476	532.864778	7.259392
6.143508	543.635750	7.264397
6.066891	552.433726	7.269402
6.395576	536.130139	7.274406
6.067123	544.763929	7.279411
6.074324	542.348915	7.284416
6.183541	546.245882	7.289421
6.068650	552.744374	7.294426
6.182051	548.222156	7.299430
6.388245	548.153368	7.304435
6.058404	530.424299	7.309440
6.186338	520.834056	7.314445
5.745604	528.475358	7.319450
6.316554	529.556614	7.324454
6.118110	543.508621	7.329459
6.075549	545.484663	7.334464
6.503076	538.542574	7.339469
6.361218	536.163934	7.344474
6.455366	515.876000	7.349478
5.788803	524.248669	7.354483
5.911119	516.293113	7.359488
5.957164	510.196722	7.364493
5.820044	514.393265	7.369498
5.772778	534.373758	7.374502
5.740861	537.174488	7.379507
6.045457	541.695926	7.384512
5.903487	536.928624	7.389517
5.972540	538.350711	7.394522
6.469771	544.778035	7.399526
6.298632	555.581345	7.404531
6.671755	546.471081	7.409536
6.417610	535.911623	7.414541
6.360213	534.459620	7.419546
6.212526	517.883557	7.424550
6.040285	519.961036	7.429555
6.082134	519.101642	7.434560
6.267917	515.576434	7.439565
6.002669	515.922171	7.444570
6.155435	513.966623	7.449574
6.083246	514.296340	7.454579
6.210401	520.278997	7.459584
5.869638	511.742817	7.464589
5.761461	514.306643	7.469594
6.216026	530.045723	7.474598
6.075447	542.841873	7.479603
6.200054	541.170371	7.484608
6.601188	545.753105	7.489613
5.854014	522.738112	7.494618
6.005021	519.768958	7.499622
6.101842	530.613110	7.504627
6.378540	528.789011	7.509632
6.095059	521.738010	7.514637
5.703692	521.588910	7.519642
6.264818	526.677945	7.524646
6.228924	545.739066	7.529651
6.233938	534.323750	7.534656
5.937990	529.530101	7.539661
6.020936	536.928397	7.544666
6.215508	534.959229	7.549670
6.121822	545.631443	7.554675
6.222848	537.470242	7.559680
6.138943	522.608056	7.564685
5.941741	517.406327	7.569690
5.870113	524.562603	7.574694
6.008039	547.649401	7.579699
6.304941	545.119031	7.584704
6.159804	552.026422	7.589709
6.177075	538.831082	7.594714
6.178190	540.680531	7.599718
6.482646	561.087637	7.604723
6.294850	528.200232	7.609728
6.274669	522.335476	7.614733
6.096137	518.751788	7.619738
6.224738	507.831551	7.624742
5.849185	520.661974	7.629747
6.014456	500.558239	7.634752
5.915705	509.149808	7.639757
5.867278	519.534735	7.644762
6.293251	526.620127	7.649766
6.330143	539.189534	7.654771
5.975120	522.832908	7.659776
6.080225	527.202425	7.664781
5.906212	531.324959	7.669786
6.405424	532.672112	7.674790
5.866657	534.044291	7.679795
6.314483	530.408098	7.684800
6.176787	529.881250	7.689805
6.023102	525.751829	7.694810
6.019525	515.998735	7.699814
6.125084	532.793010	7.704819
6.097272	530.814421	7.709824
6.332314	536.131673	7.714829
5.897293	525.681432	7.719834
6.348968	528.369590	7.724838
6.065676	535.904768	7.729843
6.218019	517.957417	7.734848
5.816992	528.765945	7.739853
5.984600	536.945325	7.744858
6.375616	535.266301	7.749862
6.274648	545.938239	7.754867
6.612235	538.696495	7.759872
6.391941	514.268991	7.764877
6.145658	519.464124	7.769882
6.362982	509.887430	7.774886
5.798030	517.191524	7.779891
6.201651	522.960384	7.784896
5.960221	510.728485	7.789901
6.004088	512.568202	7.794906
6.074465	515.182827	7.799910
5.919166	511.741018	7.804915
5.924375	508.985184	7.809920
6.060179	509.060623	7.814925
5.881597	513.708071	7.819930
6.312334	523.651746	7.824934
5.921036	524.995706	7.829939
6.204537	533.494819	7.834944
6.550619	537.208799	7.839949
5.957402	514.252531	7.844954
6.338765	510.248090	7.849958
5.917443	529.417181	7.854963
6.014607	515.753752	7.859968
5.600274	523.054860	7.864973
5.762301	543.367486	7.869978
6.050464	542.242941	7.874982
6.170523	558.338134	7.879987
6.270390	546.814593	7.884992
6.268538	549.960294	7.889997
5.767319	553.612446	7.895002
6.359782	546.084798	7.900006
6.385116	555.536499	7.905011
5.959790	550.226641	7.910016
6.381270	539.972553	7.915021
6.302487	552.692498	7.920026
6.615341	546.142477	7.925030
6.173434	534.450785	7.930035
5.871946	510.704611	7.935040
5.889954	518.622303	7.940045
5.684626	516.299537	7.945050
6.288920	530.186061	7.950054
6.303055	547.809873	7.955059
6.000350	548.776828	7.960064
6.308636	552.345027	7.965069
6.051944	549.003330	7.970074
6.080176	532.315012	7.975078
5.730804	540.662305	7.980083
6.175289	545.126885	7.985088
6.146744	546.815789	7.990093
5.870649	548.724762	7.995098
6.273977	542.784289	8.000102
6.237654	546.344717	8.005107
6.262971	552.943162	8.010112
6.060721	547.411342	8.015130
6.256798	537.159967	8.020147
6.242175	544.191088	8.025165
5.966041	553.294349	8.030182
6.029653	543.397569	8.035200
6.183303	549.893606	8.040218
6.121703	551.216724	8.045235
6.103538	546.707663	8.050253
6.343534	547.595290	8.055270
6.387723	546.550812	8.060288
6.382725	542.347487	8.065306
5.742721	526.923652	8.070323
5.958945	540.699394	8.075341
6.192894	551.387410	8.080358
6.350315	546.109129	8.085376
6.144135	552.904543	8.090394
6.035354	548.987997	8.095411
6.695149	554.743440	8.100429
6.635742	546.203233	8.105446
6.174652	534.538327	8.110464
6.114303	523.597203	8.115482
6.190084	519.191400	8.120499
6.390193	519.898746	8.125517
6.021094	526.454000	8.130534
6.009265	523.509426	8.135552
6.295250	536.866043	8.140570
6.255693	547.221674	8.145587
6.313963	537.443276	8.150605
6.291810	540.251401	8.155622
6.503886	542.447117	8.160640
6.273191	526.887841	8.165658
6.073023	527.603473	8.170675
6.142609	528.915242	8.175693
6.305116	539.857429	8.180710
6.543943	538.368665	8.185728
6.239025	525.203455	8.190746
6.207434	531.624902	8.195763
6.785211	535.156749	8.200781
6.066896	526.245223	8.205798
6.113365	520.788771	8.210816
6.388609	533.032918	8.215834
6.147878	536.666964	8.220851
6.265768	547.576970	8.225869
6.521174	553.191802	8.230886
6.451725	547.424641	8.235904
6.569929	542.386653	8.240922
6.485407	527.555233	8.245939
6.116031	509.006614	8.250957
6.222853	530.625692	8.255974
6.405197	548.998821	8.260992
6.286416	539.496185	8.266010
6.405574	559.492433	8.271027
6.497970	546.659597	8.276045
6.348224	559.509518	8.281062
6.437499	552.522076	8.286080
6.760726	548.055988	8.291098
6.301378	534.229028	8.296115
6.232310	527.087683	8.301133
6.048007	536.626060	8.306150
6.360481	542.866958	8.311168
6.493985	541.127445	8.316186
6.263043	558.003058	8.321203
6.538214	543.241585	8.326221
6.186200	547.357610	8.331238
6.176182	550.443302	8.336256
6.599184	550.327163	8.341274
6.544222	554.991323	8.346291
6.652975	550.237120	8.351309
6.600773	555.823471	8.356326
6.623362	548.424794	8.361344
6.870499	551.574366	8.366362
6.513923	554.148152	8.371379
6.598643	556.137108	8.376397
6.474815	542.796810	8.381414
6.382952	536.695336	8.386432
6.751238	542.438625	8.391450
6.493719	540.083455	8.396467
6.598490	534.980183	8.401485
6.310866	526.876832	8.406502
6.624766	545.473442	8.411520
6.457887	537.225945	8.416538
6.337874	538.682016	8.421555
6.662804	542.322171	8.426573
6.725251	546.952460	8.431590
6.644079	552.247988	8.436608
6.683613	524.918975	8.441626
6.243810	521.995923	8.446643
6.649521	538.666819	8.451661
7.065847	527.931014	8.456678
6.386163	524.291754	8.461696
6.482123	515.789950	8.466714
6.133894	522.787135	8.471731
6.648381	535.117412	8.476749
6.652717	537.508645	8.481766
6.519020	545.502067	8.486784
7.008700	542.621237	8.491802
6.976682	543.946649	8.496819
6.403941	522.154334	8.501837
6.581501	520.021008	8.506854
6.493417	539.776534	8.511872
6.926893	539.264749	8.516890
6.358917	530.193660	8.521907
6.633074	539.458875	8.526925
6.845498	541.608087	8.531942
6.289202	550.730090	8.536960
6.697347	545.688075	8.541978
6.467276	544.814878	8.546995
6.751389	550.002511	8.552013
7.042158	546.541683	8.557030
6.452370	545.155212	8.562048
6.705091	547.021049	8.567066
6.759035	550.179126	8.572083
6.537996	545.670528	8.577101
6.368748	536.225830	8.582119
6.511453	548.618442	8.587136
6.512879	543.296762	8.592154
6.273726	546.613487	8.597171
6.651200	549.601292	8.602189
6.695298	547.895742	8.607207
6.711054	556.114914	8.612224
6.396805	546.878288	8.617242
6.521114	559.228780	8.622259
6.914103	560.403464	8.627277
7.093382	563.959842	8.632295
6.570728	565.815359	8.637312
6.995001	554.044868	8.642330
6.626914	544.867328	8.647347
6.453729	554.787954	8.652365
6.826752	562.286215	8.657383
6.952814	573.417187	8.662400
6.929249	581.235964	8.667418
7.161582	575.710498	8.672435
6.833533	552.288948	8.677453
6.907803	546.662178	8.682471
6.752689	558.871285	8.687488
7.026568	552.288288	8.692506
6.765807	540.968247	8.697523
6.656889	550.178589	8.702541
6.851522	554.557850	8.707559
6.912743	549.561553	8.712576
6.829406	547.449393	8.717594
6.777062	554.368273	8.722611
6.896904	560.567207	8.727629
6.860829	559.264885	8.732647
6.826033	572.615401	8.737664
6.754574	578.508917	8.742682
7.058971	580.558897	8.747699
6.574090	576.546555	8.752717
7.289592	579.253551	8.757735
6.769827	584.865221	8.762752
7.470278	573.848227	8.767770
6.799501	566.921433	8.772787
6.821007	553.985663	8.777805
7.088872	548.538963	8.782823
6.838622	557.343028	8.787840
6.968790	556.509393	8.792858
6.794638	556.409867	8.797875
7.084880	568.423067	8.802893
7.291881	565.708706	8.807911
6.601231	558.584453	8.812928
6.881901	552.879191	8.817946
6.920403	565.874351	8.822963
7.026090	575.972778	8.827981
7.072260	570.491953	8.832999
6.720115	575.603477	8.838016
6.840824	564.536358	8.843034
6.844039	576.283970	8.848051
6.685258	577.938736	8.853069
6.859339	568.793804	8.858087
6.898744	579.463311	8.863104
6.976468	582.322839	8.868122
7.075824	576.651074	8.873139
6.883241	581.027022	8.878157
7.056499	567.705606	8.883175
6.585837	575.966301	8.888192
6.739188	573.825159	8.893210
6.881649	580.526266	8.898227
6.931356	608.607437	8.903245
7.424123	591.479615	8.908263
7.534457	614.636900	8.913280
7.397306	597.555306	8.918298
7.212042	586.215473	8.923315
6.986233	583.030812	8.928333
7.156071	581.750059	8.933351
7.017822	576.062354	8.938368
6.969037	576.951160	8.943386
7.040069	588.831639	8.948403
7.172758	596.462331	8.953421
7.175677	599.087029	8.958439
7.134890	601.257428	8.963456
7.386454	600.251693	8.968474
7.598805	584.646008	8.973491
7.056879	587.943893	8.978509
7.287896	580.264743	8.983527
6.760674	578.513572	8.988544
7.138265	580.525870	8.993562
6.885474	586.479959	8.998579
7.170905	605.463849	9.003597
7.327525	609.855509	9.008615
7.149676	613.601401	9.013632
7.357511	612.174237	9.018650
7.382313	612.748582	9.023667
7.392411	619.331548	9.028685
7.463769	598.178304	9.033703
7.187708	598.872432	9.038720
6.976180	594.148412	9.043738
7.078047	593.765820	9.048755
7.507746	603.444456	9.053773
7.863405	601.045612	9.058791
7.218016	605.577285	9.063808
7.269847	583.702334	9.068826
7.278376	580.379361	9.073843
7.073051	592.737316	9.078861
7.096943	573.794168	9.083879
6.916628	595.952126	9.088896
7.173907	607.502098	9.093914
7.530776	608.692497	9.098931
7.634979	622.635319	9.103949
7.377911	613.854269	9.108967
7.547956	616.726002	9.113984
7.656382	609.117283	9.119002
6.974880	588.768843	9.124019
7.083393	597.139308	9.129037
7.487052	596.185688	9.134055
7.197279	611.753039	9.139072
7.287705	612.913468	9.144090
7.537613	605.963420	9.149107
7.217996	616.023615	9.154125
7.468801	608.670840	9.159143
7.603733	612.902732	9.164160
7.506091	608.378446	9.169178
7.649261	612.252748	9.174195
7.262602	617.015826	9.179213
7.461231	616.617932	9.184231
7.743140	610.949838	9.189248
7.261643	608.985735	9.194266
7.399008	606.978503	9.199283
7.387873	612.235515	9.204301
7.605291	606.817206	9.209319
7.261743	608.792116	9.214336
7.411117	623.841623	9.219354
7.591564	612.709196	9.224371
7.429077	615.830823	9.229389
7.492617	621.037906	9.234407
7.668668	613.534522	9.239424
7.491254	623.800115	9.244442
7.581828	609.582171	9.249459
7.168244	625.152480	9.254477
7.456718	614.481829	9.259495
7.051515	612.569277	9.264512
7.047302	617.067817	9.269530
7.530613	613.311330	9.274547
7.291063	620.737164	9.279565
7.591171	617.163775	9.284583
7.365648	601.741140	9.289600
7.134831	614.758608	9.294618
7.765783	618.121483	9.299635
7.374580	623.707296	9.304653
7.680647	625.782690	9.309671
7.733421	624.810494	9.314688
7.638977	634.742170	9.319706
7.843258	611.584754	9.324723
7.361936	620.679156	9.329741
7.665870	619.445518	9.334759
7.598927	617.059236	9.339776
7.506881	629.259059	9.344794
7.851126	625.969557	9.349811
7.504834	629.707469	9.354829
7.669482	639.481788	9.359847
7.636018	631.672141	9.364864
7.633811	647.327511	9.369882
7.833911	640.075405	9.374899
7.689837	636.990983	9.379917
7.621808	634.815860	9.384935
7.924297	639.121230	9.389952
7.766742	629.664801	9.394970
7.882862	613.748478	9.399987
7.321143	613.057125	9.405005
7.618805	614.467011	9.410023
8.126141	632.373821	9.415040
7.756832	628.714143	9.420058
7.894835	622.551720	9.425075
7.291528	616.122019	9.430093
7.659461	630.537305	9.435111
7.433831	649.892164	9.440128
7.463144	636.293550	9.445146
8.048636	644.411434	9.450163
8.033816	648.551374	9.455181
8.131706	655.629294	9.460199
7.967378	651.171320	9.465216
7.340312	649.316290	9.470234
7.655832	638.183664	9.475251
7.862797	645.414191	9.480269
7.974732	658.010558	9.485287
8.117944	636.617578	9.490304
7.813230	653.446936	9.495322
8.105412	646.572545	9.500339
7.527883	639.048434	9.505357
8.090301	639.855527	9.510375
8.094675	642.350195	9.515392
7.716561	634.645129	9.520410
7.471286	636.068574	9.525427
7.760044	643.791979	9.530445
7.912492	647.485756	9.535463
7.620487	648.728379	9.540480
7.774367	656.952037	9.545498
8.051948	656.407755	9.550515
7.691354	647.359696	9.555533
7.524945	657.859372	9.560551
7.945467	650.657826	9.565568
7.500510	648.679904	9.570586
7.532777	643.687279	9.575603
7.706556	648.398689	9.580621
7.905580	676.595242	9.585639
8.316654	672.862782	9.590656
8.001593	657.035973	9.595674
7.980839	656.608203	9.600691
7.782953	655.300139	9.605709
8.042188	668.036216	9.610727
8.015881	665.811780	9.615744
7.652327	661.249746	9.620762
8.101546	675.331329	9.625779
7.921075	681.933907	9.630797
7.712306	684.352998	9.635815
8.566212	681.861669	9.640832
8.310860	685.950932	9.645850
8.508828	666.296751	9.650867
8.066139	664.390486	9.655885
7.832079	649.619185	9.660903
8.230019	651.111991	9.665920
7.943414	648.001229	9.670938
7.783625	639.535815	9.675955
8.023601	652.899151	9.680973
8.392655	662.269306	9.685991
8.625129	648.078852	9.691008
7.991667	651.125295	9.696026
8.285801	648.151785	9.701043
8.239934	642.224620	9.706061
7.818624	641.904768	9.711079
8.067563	644.240048	9.716096
8.012028	646.581460	9.721114
8.397519	640.617257	9.726131
8.598642	644.736861	9.731149
8.140093	640.221037	9.736167
8.452793	633.522950	9.741184
7.983074	646.092323	9.746202
7.877327	642.043092	9.751219
8.271664	639.264794	9.756237
7.993436	642.443932	9.761255
8.050032	642.699699	9.766272
8.094105	638.481055	9.771290
8.108943	648.729851	9.776307
8.370947	656.473921	9.781325
8.295037	668.469967	9.786343
8.259461	661.308658	9.791360
8.278400	668.852299	9.796378
8.527491	673.509940	9.801395
8.014710	641.897746	9.806413
8.180158	649.343066	9.811431
8.495249	662.790633	9.816448
8.127802	662.529780	9.821466
8.375656	667.467195	9.826483
8.561539	661.338273	9.831501
7.960561	658.236752	9.836519
8.430874	669.231884	9.841536
8.464400	673.496492	9.846554
8.524100	663.625965	9.851571
8.311842	653.466692	9.856589
8.436083	647.577936	9.861607
8.260852	637.945029	9.866624
7.920015	649.528237	9.871642
8.266725	667.229099	9.876659
8.371221	660.948304	9.881677
8.422800	683.004201	9.886695
8.345028	675.330077	9.891712
8.209034	674.999091	9.896730
8.410520	680.800995	9.901747
8.545615	674.736945	9.906765
8.415296	680.961228	9.911783
8.506850	684.878619	9.916800
8.420690	675.717291	9.921818
8.465526	682.306942	9.926835
8.389852	672.253112	9.931853
8.231132	684.022351	9.936871
8.567590	672.432391	9.941888
8.342612	676.440958	9.946906
8.429727	672.568371	9.951923
8.595061	677.156702	9.956941
8.475642	686.006431	9.961959
8.919894	680.341104	9.966976
8.491606	686.442124	9.971994
8.485614	674.813694	9.977011
8.660567	671.049698	9.982029
8.660147	682.721234	9.987047
8.662600	666.910336	9.992064
8.511140	678.845169	9.997082
8.739766	669.049459	10.002099
8.806583	675.992000	10.007117
8.519229	666.357922	10.012135
8.485086	662.608112	10.017152
8.462133	675.081242	10.022170
8.492843	669.416260	10.027187
8.481557	676.975036	10.032205
8.645837	682.203871	10.037223
8.453833	676.289034	10.042240
8.106749	680.268873	10.047258
8.020592	675.091812	10.052275
8.624105	677.123667	10.057293
8.317659	679.666163	10.062311
8.399089	677.229668	10.067328
8.569091	679.531846	10.072346
8.529164	678.961307	10.077363
8.893132	687.424522	10.082381
8.852524	691.714277	10.087399
8.665871	681.838887	10.092416
8.466831	689.298111	10.097434
8.907714	684.748675	10.102451
8.773417	675.622561	10.107469
8.440222	682.804896	10.112487
8.580350	689.693309	10.117504
9.049692	706.947557	10.122522
8.987543	695.541244	10.127539
8.814557	679.316399	10.132557
8.362454	690.556088	10.137575
8.690367	691.116460	10.142592
8.749382	708.125881	10.147610
8.851789	705.330177	10.152627
8.916062	702.729027	10.157645
8.886125	708.716794	10.162663
9.207939	697.783047	10.167680
8.805988	691.894534	10.172698
8.570659	689.892003	10.177715
8.648257	684.167702	10.182733
8.808139	695.263258	10.187751
8.960844	697.771014	10.192768
8.865635	694.664236	10.197786
8.864378	684.314296	10.202803
9.382172	682.553281	10.207821
8.735859	679.704672	10.212839
9.075548	673.110847	10.217856
8.801785	674.626781	10.222874
8.798598	673.103800	10.227891
8.887096	668.093608	10.232909
8.599615	670.136904	10.237927
8.852337	679.184234	10.242944
9.045329	701.685004	10.247962
8.993845	694.858036	10.252979
9.062205	691.966405	10.257997
9.064873	693.694779	10.263015
9.264480	678.419486	10.268032
9.502241	681.742353	10.273050
9.242825	685.605560	10.278067
8.986059	671.098471	10.283085
8.766614	677.250785	10.288103
8.908336	671.037245	10.293120
8.527756	666.107622	10.298138
8.438732	678.674236	10.303155
8.858184	681.710238	10.308173
9.046118	704.379139	10.313191
9.267482	709.095496	10.318208
9.010842	699.981516	10.323226
8.789268	703.935109	10.328243
9.289795	707.120285	10.333261
9.140247	713.764017	10.338279
9.272970	706.190598	10.343296
9.545648	710.206975	10.348314
9.012848	695.680826	10.353331
9.067234	682.377970	10.358349
9.032823	684.616999	10.363367
9.191965	676.574161	10.368384
8.853964	689.122786	10.373402
8.891001	699.073910	10.378419
9.278581	693.296806	10.383437
9.119816	696.678610	10.388455
9.241924	703.593822	10.393472
9.283488	706.687060	10.398490
9.098551	700.113398	10.403507
9.458220	700.256791	10.408525
9.112223	711.359397	10.413543
9.388923	701.465680	10.418560
9.712129	697.037242	10.423578
9.122711	680.720712	10.428595
9.358986	682.467064	10.433613
9.070486	686.052947	10.438631
8.830961	671.902781	10.443648
8.897582	688.554792	10.448666
8.784653	700.491442	10.453683
8.852357	703.538439	10.458701
8.618527	709.313098	10.463719
9.083724	709.718625	10.468736
9.425752	703.729599	10.473754
9.289810	702.360319	10.478771
9.507165	707.728297	10.483789
9.624707	705.610866	10.488807
9.192472	702.376844	10.493824
9.257386	698.165957	10.498842
9.330468	709.334813	10.503859
9.248522	699.213314	10.508877
9.248356	705.873982	10.513895
9.295190	706.565730	10.518912
9.439139	700.966062	10.523930
9.165609	708.827786	10.528947
9.347259	706.562091	10.533965
9.285193	702.686497	10.538983
9.016921	715.344069	10.544000
9.497535	723.974410	10.549018
9.393853	738.489776	10.554035
9.968030	740.152446	10.559053
9.461154	719.525808	10.564071
9.343961	713.836541	10.569088
9.643615	699.471091	10.574106
9.498145	698.022398	10.579123
9.826097	695.495368	10.584141
9.429191	701.104491	10.589159
9.430861	706.738676	10.594176
9.542240	699.441767	10.599194
9.402830	694.393358	10.604211
9.665683	707.234951	10.609229
9.659989	699.301117	10.614247
9.187437	698.771270	10.619264
9.440547	704.520664	10.624282
9.105706	705.261019	10.629299
9.517540	722.235276	10.634317
9.665731	737.485543	10.639335
9.459107	734.260089	10.644352
9.378531	735.620800	10.649370
9.570437	736.639198	10.654387
9.949264	735.511065	10.659405
9.711907	742.162727	10.664423
9.428701	735.332407	10.669440
9.813648	738.012970	10.674458
9.630977	740.926285	10.679475
9.836355	741.153532	10.684493
9.974721	735.240464	10.689511
9.736078	726.451089	10.694528
9.563503	714.386959	10.699546
9.312495	720.347595	10.704563
9.328371	730.617235	10.709581
9.415135	732.700740	10.714599
9.378789	738.828036	10.719616
9.310712	740.872084	10.724634
9.579913	734.204071	10.729651
9.677852	749.344763	10.734669
9.546856	744.629038	10.739687
9.384245	735.971750	10.744704
10.152219	744.532769	10.749722
9.865584	743.695379	10.754739
9.785344	735.931196	10.759757
10.106997	741.992740	10.764775
9.701422	737.764040	10.769792
9.810298	741.279249	10.774810
9.680621	750.357832	10.779827
10.011275	736.559656	10.784845
10.225229	740.063995	10.789863
10.028143	741.688009	10.794880
10.294053	734.106048	10.799898
9.976713	742.783438	10.804915
10.048311	736.421353	10.809933
10.274471	738.500127	10.814951
10.092739	732.333422	10.819968
9.773853	733.623004	10.824986
9.922902	738.322095	10.830003
9.934972	730.591471	10.835021
9.865460	735.765374	10.840039
9.554025	741.558479	10.845056
9.965942	734.639759	10.850074
9.705204	740.984615	10.855091
9.763911	736.766773	10.860109
9.789034	742.598140	10.865127
9.571862	733.182005	10.870144
9.686688	740.283538	10.875162
9.828707	742.553841	10.880179
9.665460	735.178305	10.885197
9.792994	736.105391	10.890215
9.679963	744.048857	10.895232
10.061540	744.816661	10.900250
10.202071	757.637967	10.905267
10.255468	764.975113	10.910285
9.906538	743.193422	10.915303
10.217320	759.504923	10.920320
10.289388	752.909136	10.925338
9.867253	736.444749	10.930355
9.956284	754.714276	10.935373
10.120299	755.241806	10.940391
9.961360	756.333928	10.945408
10.101788	751.762779	10.950426
10.122505	755.017022	10.955443
10.271727	762.645458	10.960461
10.547913	756.083151	10.965479
10.161168	754.748523	10.970496
10.146256	743.234879	10.975514
10.091585	735.972084	10.980531
9.985557	737.131923	10.985549
10.228556	740.336145	10.990567
10.079298	761.535847	10.995584
10.523489	755.488390	11.000602
10.423336	754.766218	11.005619
10.225941	758.771822	11.010637
10.522472	741.484764	11.015655
10.097550	738.493476	11.020672
10.278607	737.924598	11.025690
10.285328	744.200754	11.030707
10.329233	731.624056	11.035725
10.381269	738.789499	11.040743
10.123952	745.853241	11.045760
9.921713	735.824024	11.050778
9.825836	739.948353	11.055795
10.158344	755.084927	11.060813
10.629070	755.891828	11.065831
10.400691	761.859368	11.070848
10.482965	767.715743	11.075866
10.528094	760.781654	11.080883
10.601861	759.269861	11.085901
10.501518	752.613902	11.090919
10.141107	747.110063	11.095936
10.155395	732.349993	11.100954
10.588822	750.748394	11.105971
10.585284	758.530493	11.110989
10.465806	740.829204	11.116007
10.204502	744.201886	11.121024
10.413622	758.220093	11.126042
10.493287	749.845829	11.131059
10.385644	752.655230	11.136077
10.622886	757.404799	11.141095
10.335111	750.955962	11.146112
10.386500	755.274126	11.151130
10.499039	757.866172	11.156147
10.211426	754.522232	11.161165
10.925393	754.629317	11.166183
10.836244	757.651468	11.171200
10.495863	744.927674	11.176218
10.133780	738.927457	11.181235
10.538145	751.907679	11.186253
10.476557	758.634612	11.191271
9.974681	764.087908	11.196288
10.438203	771.183300	11.201306
10.893754	764.037516	11.206323
10.516282	766.995033	11.211341
10.349734	767.172936	11.216359
10.058227	762.550942	11.221376
10.548383	771.244188	11.226394
10.656575	774.361069	11.231411
10.521986	772.057189	11.236429
10.693562	766.712430	11.241447
10.443248	765.237758	11.246464
10.695352	767.249268	11.251482
10.871389	760.569184	11.256499
10.477098	770.505724	11.261517
10.742469	757.521217	11.266535
10.709962	761.978519	11.271552
10.562396	765.777109	11.276570
10.652623	764.848016	11.281587
10.641853	763.170403	11.286605
10.572742	769.011842	11.291623
10.625115	781.889363	11.296640
10.602354	795.987354	11.301658
10.809664	792.808913	11.306675
11.014935	807.077755	11.311693
10.871782	797.810046	11.316711
10.946247	804.332168	11.321728
10.843786	796.099669	11.326746
11.092525	787.578077	11.331763
10.814798	772.124534	11.336781
11.039923	763.171802	11.341799
10.893882	762.745052	11.346816
10.840883	758.531001	11.351834
11.229346	760.514663	11.356851
10.914675	760.680141	11.361869
11.110842	764.815063	11.366887
10.853488	763.477257	11.371904
10.537962	765.258320	11.376922
10.861855	756.122274	11.381939
10.591673	769.595702	11.386957
10.933471	776.083869	11.391975
10.504001	784.926930	11.396992
10.888483	790.707984	11.402010
11.419032	793.077935	11.407027
11.131699	803.504403	11.412045
11.230075	787.676546	11.417063
10.824814	785.679745	11.422080
11.053856	770.790663	11.427098
10.892088	765.002365	11.432115
10.665784	785.531694	11.437133
10.840693	787.737918	11.442151
11.085832	792.327954	11.447168
11.002332	799.872056	11.452186
11.070273	791.554126	11.457203
11.150785	796.572279	11.462221
11.600757	791.340630	11.467239
11.278307	788.773850	11.472256
11.016175	787.816780	11.477274
11.461917	784.528284	11.482291
11.291407	771.086762	11.487309
11.137800	767.130234	11.492327
10.850155	757.770997	11.497344
11.005644	761.008775	11.502362
11.297298	776.794126	11.507379
10.816174	786.054997	11.512397
10.928497	793.441267	11.517415
10.931857	792.207591	11.522432
10.960753	792.641135	11.527450
11.479019	788.896543	11.532467
10.948003	790.802474	11.537485
11.127475	788.329390	11.542503
11.132388	786.338021	11.547520
10.862683	787.284504	11.552538
11.019568	790.958787	11.557555
11.042773	787.732145	11.562573
10.988550	793.509236	11.567591
11.307984	806.444397	11.572608
11.658086	809.125220	11.577626
11.379098	803.399086	11.582643
11.324316	799.812662	11.587661
11.520577	796.626896	11.592679
11.188070	792.390928	11.597696
11.116843	785.965138	11.602714
11.452961	803.931047	11.607731
11.393293	806.631367	11.612749
11.440543	812.755605	11.617767
11.615482	813.481688	11.622784
11.361504	799.053137	11.627802
11.400075	799.662706	11.632819
11.430160	804.197259	11.637837
11.371640	810.581646	11.642855
11.806631	823.104688	11.647872
11.208945	807.343421	11.652890
11.772475	803.451411	11.657907
11.491955	794.460885	11.662925
11.453754	791.274896	11.667943
11.420386	785.393042	11.672960
11.482906	800.922146	11.677978
11.454209	802.158367	11.682995
11.321252	816.523949	11.688013
11.413121	813.425988	11.693031
11.417989	820.914461	11.698048
11.170900	819.656139	11.703066
11.895579	810.716675	11.708083
11.638396	824.592357	11.713101
11.644934	822.212991	11.718119
11.641090	825.194488	11.723136
11.769778	815.920619	11.728154
12.188243	820.305282	11.733171
11.914579	825.811126	11.738189
11.701800	806.385933	11.743207
11.503003	802.943365	11.748224
11.301428	797.807772	11.753242
11.758287	807.665381	11.758259
11.963241	816.991502	11.763277
11.695722	819.410090	11.768295
11.824483	815.449497	11.773312
11.625168	829.540874	11.778330
12.151447	808.233832	11.783347
11.807415	807.898253	11.788365
11.653819	792.917195	11.793383
11.749670	784.743349	11.798400
11.556505	787.920957	11.803418
11.681365	800.718614	11.808435
11.734962	815.410977	11.813453
11.742833	820.582749	11.818471
11.823696	808.158809	11.823488
11.811502	817.571692	11.828506
11.988353	808.224427	11.833523
11.559979	821.943391	11.838541
11.836641	814.823209	11.843559
12.026129	808.821366	11.848576
11.727149	825.567499	11.853594
11.854250	803.224566	11.858611
12.246263	811.477151	11.863629
11.809458	812.287796	11.868647
11.859009	816.998629	11.873664
11.793514	817.681194	11.878682
11.838385	812.094808	11.883699
11.687196	810.854295	11.888717
11.548222	818.862311	11.893735
11.784021	807.136256	11.898752
11.665675	812.921195	11.903770
12.031945	814.396126	11.908787
12.107212	818.268810	11.913805
11.907047	820.247901	11.918823
11.886711	808.816291	11.923840
11.936047	823.583860	11.928858
12.219190	836.953902	11.933875
12.086193	832.235725	11.938893
12.143932	838.259832	11.943911
12.395472	826.452927	11.948928
11.798371	828.145711	11.953946
12.188876	824.008029	11.958963
11.983933	836.894955	11.963981
12.040680	849.525792	11.968999
12.412314	849.096646	11.974016
12.079549	845.406570	11.979034
12.458349	842.414407	11.984051
12.132153	838.342609	11.989069
12.256753	822.502706	11.994087
12.276233	814.710983	11.999104
11.775198	821.595194	12.004122
12.215126	842.113105	12.009139
12.482812	846.838678	12.014157
12.453336	841.599940	12.019175
12.530793	844.706858	12.024192
11.976366	825.609113	12.029210
12.102676	827.914892	12.034227
12.550403	840.764622	12.039245
12.388529	834.017141	12.044263
12.366378	819.912398	12.049280
12.285920	826.355524	12.054298
12.082099	837.065404	12.059315
12.439647	844.737393	12.064333
12.371791	848.356916	12.069351
12.669827	846.182282	12.074368
12.434430	833.586708	12.079386
12.762860	825.398221	12.084403
12.202263	812.777187	12.089421
11.813174	813.233652	12.094439
12.185195	821.627316	12.099456
12.278363	842.404167	12.104474
12.369425	837.978231	12.109491
12.543718	834.421156	12.114509
12.175175	835.331327	12.119527
12.411583	843.739345	12.124544
11.969468	851.318624	12.129562
12.312160	842.736406	12.134579
12.403713	844.744837	12.139597
12.300281	843.566101	12.144615
12.442967	850.251248	12.149632
12.254516	855.697262	12.154650
12.679448	872.138614	12.159667
12.605877	883.621148	12.164685
12.329979	886.290298	12.169703
12.729198	880.914179	12.174720
12.356613	872.953106	12.179738
12.492305	882.578260	12.184755
12.609290	872.533693	12.189773
12.319601	883.337406	12.194791
12.917666	870.673447	12.199808
12.490002	880.442080	12.204826
12.756973	878.277003	12.209843
12.997083	878.206833	12.214861
12.961394	882.540013	12.219879
13.208550	880.088893	12.224896
12.956928	879.793739	12.229914
12.881993	868.936162	12.234931
12.922190	857.352019	12.239949
12.519864	861.591479	12.244967
12.775576	841.231203	12.249984
12.399105	848.090117	12.255002
12.785910	864.235356	12.260019
12.887523	866.475059	12.265037
12.641578	878.634382	12.270055
12.915569	860.728587	12.275072
12.492628	867.648133	12.280090
12.895124	868.474483	12.285107
13.168172	869.704341	12.290125
12.846328	878.338169	12.295143
12.935840	863.499217	12.300160
12.824679	879.294557	12.305178
12.857686	874.775665	12.310195
12.800785	872.804832	12.315213
12.797853	880.466541	12.320231
13.066937	873.665145	12.325248
12.756764	871.636087	12.330266
12.795490	869.777184	12.335283
13.204957	869.453970	12.340301
12.975215	881.309885	12.345319
13.068313	865.026308	12.350336
12.967630	866.221684	12.355354
12.766336	873.897964	12.360371
13.339498	872.966013	12.365389
13.176796	872.417921	12.370407
13.011160	867.540786	12.375424
13.017447	881.014875	12.380442
13.026947	879.890788	12.385459
13.151870	879.193608	12.390477
12.832844	873.988931	12.395495
13.035289	872.124623	12.400512
13.143105	874.057746	12.405530
12.920898	866.840191	12.410547
12.870611	870.959874	12.415565
13.324020	888.123374	12.420583
13.309817	887.499472	12.425600
13.259079	880.497427	12.430618
13.286975	869.684754	12.435635
13.530198	861.070251	12.440653
13.163853	883.532150	12.445671
13.347170	880.021399	12.450688
13.435826	862.651847	12.455706
13.329709	871.760263	12.460723
13.178990	864.382694	12.465741
13.280975	864.941538	12.470759
13.354123	863.730471	12.475776
13.503319	864.701811	12.480794
13.310669	867.574975	12.485811
13.624810	870.671324	12.490829
13.326813	865.505293	12.495847
13.662552	869.057536	12.500864
13.443002	867.225373	12.505882
13.428060	870.590828	12.510899
13.458650	866.226247	12.515917
13.318003	860.973497	12.520935
13.462017	869.477393	12.525952
13.771112	874.316287	12.530970
13.471594	874.645570	12.535987
13.770809	867.496544	12.541005
13.510643	871.210833	12.546023
13.733723	869.828067	12.551040
13.331496	872.637459	12.556058
13.381612	870.432052	12.561075
13.605142	870.279794	12.566093
13.279172	878.624790	12.571111
13.349029	859.747893	12.576128
13.518785	866.736392	12.581146
13.510862	880.205940	12.586163
13.441488	864.271103	12.591181
13.358767	877.811956	12.596199
13.322512	873.910798	12.601216
13.473489	871.225815	12.606234
13.660618	903.415659	12.611251
13.975019	902.449513	12.616269
13.969844	893.569698	12.621287
13.393561	873.124962	12.626304
13.526733	880.030257	12.631322
13.599321	900.563781	12.636339
14.027404	894.050513	12.641357
13.574428	907.552103	12.646375
13.681557	897.925216	12.651392
13.953032	893.404798	12.656410
13.852107	899.592033	12.661427
13.586114	896.343290	12.666445
13.704586	904.784116	12.671463
13.863591	898.549226	12.676480
14.150132	893.535757	12.681498
13.848065	899.799039	12.686515
14.337025	895.006699	12.691533
13.845317	877.062193	12.696551
13.539384	876.901779	12.701568
14.175399	879.006034	12.706586
13.743059	894.739330	12.711603
13.810545	887.272747	12.716621
14.081655	903.723512	12.721639
14.076293	900.391056	12.726656
14.325991	890.582866	12.731674
14.066318	881.905027	12.736691
13.812283	871.066417	12.741709
13.664746	861.896129	12.746727
13.689544	883.693401	12.751744
14.178764	886.003674	12.756762
13.607142	899.970257	12.761779
14.341336	894.495282	12.766797
14.096255	901.196016	12.771815
14.221436	894.207307	12.776832
14.286624	897.559724	12.781850
13.990575	897.735509	12.786867
14.387111	890.209431	12.791885
14.078264	893.505568	12.796903
13.935227	901.764647	12.801920
14.268054	900.636725	12.806938
14.260540	908.541287	12.811955
14.402214	898.418129	12.816973
14.578815	903.172254	12.821991
14.016923	876.711255	12.827008
14.076550	871.421273	12.832026
14.037138	884.107491	12.837043
14.198457	886.810275	12.842061
14.487849	899.809328	12.847079
14.390941	893.689454	12.852096
14.460921	882.443025	12.857114
13.933059	882.108595	12.862131
14.168536	888.741424	12.867149
14.385259	904.966378	12.872167
14.285964	896.082040	12.877184
14.329716	888.842960	12.882202
14.368185	896.149276	12.887219
14.761132	895.655692	12.892237
14.459122	893.537797	12.897255
14.341891	888.378100	12.902272
14.537758	894.887776	12.907290
14.218573	903.638973	12.912307
14.160593	887.030795	12.917325
14.356637	891.197951	12.922343
14.145040	895.180745	12.927360
14.506041	891.086004	12.932378
14.354147	895.057161	12.937395
14.267594	888.880863	12.942413
14.360717	890.425444	12.947431
13.950747	897.628241	12.952448
14.272985	885.266498	12.957466
14.227086	907.301922	12.962483
14.526847	912.407579	12.967501
14.907445	920.736211	12.972519
14.527737	928.504392	12.977536
14.940928	919.513602	12.982554
14.736268	904.210913	12.987571
14.562332	895.158726	12.992589
14.500265	892.719046	12.997607
14.358444	912.535201	13.002624
15.040549	916.116520	13.007642
14.589535	918.983383	13.012659
14.583744	926.511359	13.017677
14.657509	917.027843	13.022695
14.456963	924.205294	13.027712
15.015308	910.477486	13.032730
15.015464	914.896960	13.037747
15.310294	917.266128	13.042765
15.127198	905.980021	13.047783
15.107843	885.404757	13.052800
14.720599	881.938990	13.057818
14.515681	888.722829	13.062835
14.537250	881.435755	13.067853
15.011036	892.617645	13.072871
14.887034	903.778175	13.077888
15.166830	908.507375	13.082906
14.653222	898.377467	13.087923
15.050120	910.404309	13.092941
15.023101	910.374445	13.097959
14.851826	917.868455	13.102976
14.871112	902.075298	13.107994
14.979014	910.261620	13.113011
14.865430	915.050516	13.118029
15.187091	912.977658	13.123047
15.256691	916.824241	13.128064
15.301360	906.121251	13.133082
14.756059	894.560324	13.138099
14.944100	888.999849	13.143117
14.860943	897.617075	13.148135
14.724144	912.376126	13.153152
15.112006	915.440423	13.158170
14.628585	908.865119	13.163187
15.015870	922.057031	13.168205
14.900141	917.812660	13.173223
14.913377	919.004369	13.178240
15.066034	910.425865	13.183258
14.979866	913.394905	13.188275
15.139026	918.414173	13.193293
15.372121	908.399009	13.198311
15.313893	921.198386	13.203328
15.166572	908.828408	13.208346
15.037809	916.037589	13.213363
15.404003	927.687500	13.218381
15.324769	909.941674	13.223399
14.975857	920.021079	13.228416
14.914778	914.488773	13.233434
15.166725	936.688072	13.238451
15.389109	952.951504	13.243469
15.384056	938.463087	13.248487
15.254326	944.744553	13.253504
15.492676	952.609197	13.258522
15.641322	950.748063	13.263539
15.527685	958.487444	13.268557
15.646473	952.094937	13.273575
15.205960	945.271034	13.278592
15.486318	942.927192	13.283610
15.472480	947.492860	13.288627
15.658427	937.288653	13.293645
16.063571	944.641466	13.298663
15.555888	929.040759	13.303680
15.502703	916.652069	13.308698
15.408697	906.771557	13.313715
15.466607	919.237820	13.318733
15.800166	916.686211	13.323751
15.396444	928.932660	13.328768
15.466754	936.808434	13.333786
15.674479	940.189756	13.338803
15.634740	939.970000	13.343821
15.701248	943.555927	13.348839
15.339361	953.354772	13.353856
15.563101	939.647888	13.358874
15.744029	938.963495	13.363891
15.617019	947.663376	13.368909
15.732681	941.221496	13.373927
15.627318	956.523723	13.378944
15.560729	941.154585	13.383962
15.900016	942.687030	13.388979
15.920867	943.187152	13.393997
15.976185	936.609407	13.399015
16.017166	942.661812	13.404032
15.789148	951.102845	13.409050
15.861182	940.575001	13.414067
15.757613	949.489967	13.419085
15.762790	951.885258	13.424103
15.546760	942.641019	13.429120
15.721740	942.514694	13.434138
15.978751	945.556534	13.439155
15.814610	946.387961	13.444173
15.869044	942.585263	13.449191
15.805635	944.251073	13.454208
16.071904	940.604772	13.459226
16.103355	943.070117	13.464243
16.060930	948.038175	13.469261
16.129232	944.280124	13.474279
15.907242	947.894931	13.479296
16.035612	952.825910	13.484314
15.946162	940.189892	13.489331
15.603281	955.327566	13.494349
16.396554	942.026474	13.499367
16.009693	939.252241	13.504384
15.635803	947.615133	13.509402
16.091609	954.298966	13.514419
15.834850	968.161323	13.519437
16.243367	967.851746	13.524455
15.928611	974.512263	13.529472
16.312554	977.937197	13.534490
16.285981	971.806555	13.539507
16.235937	981.139883	13.544525
16.377442	968.563297	13.549543
16.084135	975.427517	13.554560
16.143047	976.645043	13.559578
16.138005	973.146995	13.564595
15.956567	983.753886	13.569613
15.866610	969.015146	13.574631
15.759553	976.834045	13.579648
16.033650	973.450373	13.584666
16.097212	976.554595	13.589683
16.286753	1007.806727	13.594701
16.633709	1010.004726	13.599719
16.728915	1011.266346	13.604736
16.281871	990.725108	13.609754
16.292594	987.907306	13.614771
16.619778	1008.736147	13.619789
17.031866	1002.539399	13.624807
16.389577	997.382490	13.629824
16.553368	979.274531	13.634842
16.444447	980.027457	13.639859
16.339634	978.065709	13.644877
16.623039	979.403393	13.649895
16.711740	988.448194	13.654912
16.914904	978.800367	13.659930
16.880099	973.816751	13.664947
16.946393	977.728254	13.669965
16.961439	966.606471	13.674983
16.535969	974.632193	13.680000
16.483459	973.343180	13.685018
16.912990	965.124331	13.690035
16.675121	971.580443	13.695053
16.746983	964.982730	13.700071
16.578822	969.032073	13.705088
16.554333	967.081458	13.710106
16.800274	959.301344	13.715123
16.747382	970.555467	13.720141
16.778320	965.663727	13.725159
16.838721	971.803568	13.730176
16.823334	967.709207	13.735194
16.922001	963.568149	13.740211
16.641308	972.695338	13.745229
16.634485	965.036210	13.750247
16.653014	964.907004	13.755264
16.685018	977.702342	13.760282
16.946399	978.751197	13.765299
16.434207	1000.287140	13.770317
16.863607	1008.059425	13.775335
16.805959	1006.899582	13.780352
16.709812	1003.292687	13.785370
17.173955	999.261962	13.790387
17.413907	1009.171193	13.795405
17.152500	1001.358876	13.800423
17.206555	1010.255603	13.805440
16.873658	1002.925293	13.810458
17.173598	991.653083	13.815475
17.087263	1003.010673	13.820493
17.329347	996.926553	13.825511
16.878636	1002.677428	13.830528
16.981251	1004.040463	13.835546
17.228582	998.300692	13.840563
16.966813	1004.597705	13.845581
16.700688	996.118766	13.850599
17.004065	998.622830	13.855616
16.781770	997.274190	13.860634
17.065207	994.417716	13.865651
16.849067	1007.831250	13.870669
17.021533	1009.600583	13.875687
17.483108	1009.303395	13.880704
17.503132	1026.053221	13.885722
17.498988	1010.026956	13.890739
17.385010	1008.551773	13.895757
17.135075	1002.021294	13.900775
17.292308	1002.465520	13.905792
17.231371	1019.527977	13.910810
17.290284	1020.265569	13.915827
17.162704	1028.232349	13.920845
17.719644	1020.633547	13.925863
17.483937	1019.026143	13.930880
17.211212	1029.320057	13.935898
17.902550	1035.838155	13.940915
17.512677	1020.234911	13.945933
17.478451	1029.050782	13.950951
17.786097	1019.983396	13.955968
17.454992	1024.611849	13.960986
17.554268	1025.769371	13.966003
17.833629	1027.175924	13.971021
17.323923	1025.480751	13.976039
17.492200	1026.100288	13.981056
17.075458	1026.643302	13.986074
17.541763	1025.082261	13.991091
17.580442	1028.082652	13.996109
17.338945	1028.388671	14.001127
17.577530	1026.012358	14.006144
17.089734	1026.055194	14.011162
17.535616	1024.012080	14.016179
17.556263	1029.607132	14.021197
17.517209	1054.670940	14.026215
17.878858	1053.913279	14.031232
17.521140	1064.567266	14.036250
18.273513	1059.806529	14.041267
17.853962	1067.314381	14.046285
17.834734	1069.676821	14.051303
17.990610	1048.408812	14.056320
17.811262	1065.258446	14.061338
17.992123	1062.446367	14.066355
18.071982	1068.297745	14.071373
17.899692	1054.991088	14.076391
18.072268	1053.405171	14.081408
17.918638	1049.633779	14.086426
17.965531	1052.791452	14.091443
18.060403	1060.462674	14.096461
17.931870	1060.141468	14.101479
17.993862	1049.515718	14.106496
17.919819	1057.242997	14.111514
18.179599	1057.210711	14.116531
17.628714	1059.679705	14.121549
17.921601	1058.937342	14.126567
17.884764	1066.762397	14.131584
17.917851	1065.634300	14.136602
17.874504	1064.500135	14.141619
17.699881	1063.503000	14.146637
17.767076	1062.380682	14.151655
17.853967	1066.829756	14.156672
17.965999	1075.141939	14.161690
18.136159	1080.566854	14.166707
18.303652	1087.959007	14.171725
18.111791	1098.881820	14.176743
18.384166	1090.136507	14.181760
18.198533	1086.677823	14.186778
18.424822	1082.992040	14.191795
18.758330	1088.343712	14.196813
18.418566	1081.840542	14.201831
18.525520	1094.657345	14.206848
18.132997	1089.608121	14.211866
18.310357	1090.345037	14.216883
18.410208	1103.394676	14.221901
18.340952	1095.413966	14.226919
18.886469	1087.581231	14.231936
18.638577	1094.383678	14.236954
18.653204	1086.129311	14.241971
18.713346	1079.901534	14.246989
18.047099	1077.374494	14.252007
18.509246	1076.214462	14.257024
18.173283	1091.074006	14.262042
18.399741	1092.555833	14.267059
18.691481	1094.989899	14.272077
18.527255	1092.755030	14.277095
18.538278	1086.131695	14.282112
18.447772	1102.052667	14.287130
18.655530	1088.479865	14.292147
18.869819	1091.650821	14.297165
18.588266	1093.939705	14.302183
18.411348	1082.859795	14.307200
18.332428	1083.141311	14.312218
18.520256	1082.374780	14.317235
18.518102	1089.815242	14.322253
18.880809	1098.624308	14.327271
19.023759	1101.248683	14.332288
18.684170	1100.702555	14.337306
18.440974	1105.495313	14.342323
18.883565	1117.057658	14.347341
18.933983	1125.243851	14.352359
19.118010	1116.040761	14.357376
18.989970	1135.708887	14.362394
19.138262	1121.465876	14.367411
18.697572	1099.423297	14.372429
19.040406	1120.634777	14.377447
19.607600	1112.025938	14.382464
18.905877	1103.264257	14.387482
18.884078	1082.882506	14.392499
18.857925	1094.939351	14.397517
19.365433	1105.294505	14.402535
19.276385	1094.758043	14.407552
19.030985	1089.967924	14.412570
18.926724	1086.529645	14.417587
19.214360	1076.357845	14.422605
18.781362	1095.940708	14.427623
19.513684	1102.266464	14.432640
19.089381	1110.748582	14.437658
19.398658	1117.880155	14.442675
19.618760	1109.054508	14.447693
19.265795	1091.283936	14.452711
18.877897	1087.519954	14.457728
18.969275	1102.400804	14.462746
18.803429	1111.393859	14.467763
19.138809	1118.376064	14.472781
19.380633	1119.390470	14.477799
19.472541	1111.455351	14.482816
19.390426	1112.268212	14.487834
19.225366	1125.813935	14.492851
19.439020	1123.406791	14.497869
19.141111	1118.094522	14.502887
19.492222	1119.588030	14.507904
19.384933	1118.982256	14.512922
19.515917	1112.777596	14.517939
19.566622	1111.118325	14.522957
19.399233	1114.790869	14.527975
19.693025	1111.086838	14.532992
19.171658	1126.093571	14.538010
19.307603	1114.765315	14.543027
19.788841	1112.760336	14.548045
19.542807	1123.605912	14.553063
19.736567	1122.469563	14.558080
19.562981	1108.890284	14.563098
19.222629	1122.101448	14.568115
19.570452	1125.067697	14.573133
19.292413	1126.498470	14.578151
19.787456	1132.291693	14.583168
19.839033	1155.472886	14.588186
19.902635	1149.106933	14.593203
19.808397	1150.741548	14.598221
19.753629	1150.957863	14.603239
19.645892	1156.135666	14.608256
20.044304	1163.970720	14.613274
20.013223	1166.265657	14.618291
19.982053	1141.735657	14.623309
19.936771	1131.887886	14.628327
19.732392	1126.997291	14.633344
19.872703	1139.045950	14.638362
20.108759	1147.844877	14.643379
19.995324	1146.978743	14.648397
20.001932	1141.780487	14.653415
20.085964	1140.035010	14.658432
19.837240	1135.334190	14.663450
19.740981	1148.325542	14.668467
20.006587	1145.214057	14.673485
19.823584	1157.228575	14.678503
20.127611	1141.526973	14.683520
19.839826	1156.446717	14.688538
19.828731	1156.218486	14.693555
19.590813	1149.341821	14.698573
19.742415	1150.503991	14.703591
19.907772	1150.446961	14.708608
20.169005	1175.018304	14.713626
19.968553	1185.873908	14.718643
20.239461	1175.046842	14.723661
20.539029	1188.437111	14.728679
20.546720	1180.800473	14.733696
20.453086	1180.403233	14.738714
20.519958	1179.292769	14.743731
20.387600	1155.571467	14.748749
20.285376	1158.137171	14.753767
20.083890	1151.416271	14.758784
20.659515	1172.153006	14.763802
20.388492	1167.097455	14.768819
20.768984	1175.605447	14.773837
20.502501	1167.979090	14.778855
20.475577	1164.453419	14.783872
20.311817	1154.650996	14.788890
20.484679	1171.619679	14.793907
20.452096	1176.189693	14.798925
20.416910	1183.108381	14.803943
20.557900	1182.803253	14.808960
20.688500	1183.084197	14.813978
20.633909	1177.768897	14.818995
20.590914	1182.640191	14.824013
20.246500	1191.154617	14.829031
20.817803	1181.111630	14.834048
20.844742	1188.341459	14.839066
20.544478	1191.058184	14.844083
20.717768	1177.866135	14.849101
20.380104	1183.331509	14.854119
21.004525	1168.581103	14.859136
20.484650	1185.310004	14.864154
20.192111	1173.613017	14.869171
20.955428	1171.910179	14.874189
20.354017	1181.525952	14.879207
20.602261	1174.092636	14.884224
21.245767	1187.696103	14.889242
20.852604	1183.768032	14.894259
20.811043	1176.735699	14.899277
20.824004	1186.798285	14.904295
21.174179	1184.131799	14.909312
20.957194	1187.492332	14.914330
20.750945	1191.177417	14.919347
21.509375	1184.759019	14.924365
21.199207	1193.387255	14.929383
21.048097	1175.584410	14.934400
20.823968	1173.018932	14.939418
21.112145	1187.397340	14.944435
21.407354	1182.187986	14.949453
21.270292	1180.108432	14.954471
20.817392	1183.895879	14.959488
21.227297	1189.157809	14.964506
21.305349	1194.878255	14.969523
21.305808	1182.726412	14.974541
21.045450	1188.629727	14.979559
21.441924	1190.632788	14.984576
21.384839	1184.469019	14.989594
20.985806	1188.634905	14.994611
21.100728	1183.797415	14.999629
21.302744	1191.689541	15.004647
20.864252	1197.736058	15.009664
21.008154	1183.127239	15.014682
21.009439	1197.480636	15.019699
21.449548	1189.842407	15.024717
21.446682	1192.138982	15.029735
21.385261	1197.650626	15.034752
21.648046	1183.342582	15.039770
21.670445	1189.633550	15.044787
21.421777	1186.599170	15.049805
21.169797	1187.786113	15.054823
21.216361	1204.843409	15.059840
21.470694	1210.040715	15.064858
21.581939	1221.623057	15.069875
21.860229	1218.757848	15.074893
21.897942	1222.746271	15.079911
21.715246	1220.893509	15.084928
22.040574	1214.558086	15.089946
22.029371	1213.694736	15.094963
21.959167	1196.938956	15.099981
21.614539	1189.979727	15.104999
21.628571	1194.591248	15.110016
21.833759	1192.095153	15.115034
21.468286	1210.817730	15.120051
21.974110	1206.507667	15.125069
21.835296	1223.034880	15.130087
21.690849	1231.028368	15.135104
22.010356	1227.133870	15.140122
21.806219	1227.935411	15.145139
21.830059	1221.195744	15.150157
22.143340	1213.014378	15.155175
21.745993	1223.079252	15.160192
21.764409	1209.880884	15.165210
22.024944	1224.506573	15.170227
21.814150	1222.474034	15.175245
22.013690	1212.902239	15.180263
21.965515	1223.069031	15.185280
21.846565	1212.531722	15.190298
22.052352	1218.380061	15.195315
22.266153	1211.768431	15.200333
22.104451	1212.882986	15.205351
21.957163	1227.733329	15.210368
22.338884	1220.984712	15.215386
21.724961	1227.696744	15.220403
22.164977	1232.802949	15.225421
22.234962	1248.355086	15.230439
22.241532	1247.202228	15.235456
22.764926	1253.445269	15.240474
22.148878	1252.685018	15.245491
22.491629	1248.828005	15.250509
22.134981	1246.999656	15.255527
22.356214	1255.130136	15.260544
22.896490	1242.015161	15.265562
22.780677	1240.123592	15.270579
22.614172	1229.051893	15.275597
22.529671	1219.121192	15.280615
22.248180	1220.989481	15.285632
22.770929	1224.857798	15.290650
22.479264	1234.004766	15.295667
22.807139	1234.660920	15.300685
22.442743	1210.112661	15.305703
22.262323	1229.696271	15.310720
22.784454	1233.704827	15.315738
22.800926	1239.086309	15.320755
22.669565	1243.204433	15.325773
22.732542	1237.308946	15.330791
22.490304	1258.349429	15.335808
22.846217	1240.612895	15.340826
22.386515	1243.851370	15.345843
22.503573	1248.222098	15.350861
22.766674	1239.977565	15.355879
22.777399	1247.846419	15.360896
23.070150	1244.929413	15.365914
23.125631	1249.912585	15.370931
22.935219	1249.859237	15.375949
23.214932	1233.834445	15.380967
23.057324	1239.433050	15.385984
23.276363	1233.181315	15.391002
22.817110	1244.672350	15.396019
22.822114	1236.641506	15.401037
22.821646	1230.998593	15.406055
22.879073	1244.997733	15.411072
22.887462	1235.188067	15.416090
23.222347	1243.091328	15.421107
23.033071	1237.487880	15.426125
23.231081	1240.285239	15.431143
22.861554	1243.450751	15.436160
22.960732	1240.933197	15.441178
23.125161	1241.967289	15.446195
23.007769	1254.113931	15.451213
23.298320	1253.892140	15.456231
23.117623	1268.631527	15.461248
23.583558	1265.580600	15.466266
22.998971	1262.933947	15.471283
23.198956	1276.299023	15.476301
23.436125	1271.453113	15.481319
23.297900	1277.037310	15.486336
23.712972	1270.170775	15.491354
23.475426	1272.614986	15.496371
23.509470	1279.609665	15.501389
23.503600	1276.566635	15.506407
23.411067	1270.829686	15.511424
23.473297	1268.459353	15.516442
23.680831	1262.092203	15.521459
23.478538	1276.209082	15.526477
23.485706	1273.354813	15.531495
23.308790	1268.644841	15.536512
23.567952	1275.303939	15.541530
23.547455	1269.536979	15.546547
23.484983	1272.013076	15.551565
23.373414	1266.562498	15.556583
23.368105	1269.530842	15.561600
23.576561	1264.159249	15.566618
23.921092	1280.741276	15.571635
23.769332	1281.626276	15.576653
23.736515	1291.017072	15.581671
23.613696	1303.249282	15.586688
23.960520	1304.551224	15.591706
24.066118	1302.518350	15.596723
23.721250	1306.445037	15.601741
24.174626	1309.663523	15.606759
24.183167	1307.440420	15.611776
24.437780	1278.719124	15.616794
24.092984	1275.995644	15.621811
23.871700	1274.856031	15.626829
23.704156	1265.677097	15.631847
23.825784	1275.248235	15.636864
23.845012	1283.633535	15.641882
23.940200	1294.341163	15.646899
24.314350	1296.835648	15.651917
24.076979	1287.686346	15.656935
24.004606	1295.113515	15.661952
24.217212	1287.763581	15.666970
24.319566	1292.399310	15.671987
23.967958	1299.040469	15.677005
24.023606	1291.168524	15.682023
23.861306	1308.660192	15.687040
24.478398	1294.185442	15.692058
24.311308	1293.730073	15.697075
24.303574	1298.936469	15.702093
24.511494	1294.218988	15.707111
24.356268	1304.662540	15.712128
24.446668	1296.940928	15.717146
24.587987	1287.366111	15.722163
24.229615	1294.045585	15.727181
24.376218	1299.916135	15.732199
24.610716	1309.489506	15.737216
24.547091	1331.259511	15.742234
24.615387	1329.590618	15.747251
24.699354	1335.764008	15.752269
24.904406	1327.416439	15.757287
24.772598	1320.722329	15.762304
24.463772	1312.953510	15.767322
24.859396	1314.978379	15.772339
24.620331	1321.476166	15.777357
24.590213	1322.788439	15.782375
24.844768	1327.019754	15.787392
24.877069	1325.806347	15.792410
24.758039	1329.903365	15.797427
24.761635	1327.994415	15.802445
24.867340	1328.191300	15.807463
25.165536	1326.442099	15.812480
24.936935	1326.975091	15.817498
25.207447	1319.153045	15.822515
25.282846	1322.355268	15.827533
25.272483	1316.869447	15.832551
24.881285	1301.652592	15.837568
24.914118	1304.579998	15.842586
25.104888	1299.526622	15.847603
24.791295	1309.986507	15.852621
25.266000	1315.031898	15.857639
25.309021	1316.400972	15.862656
25.082297	1318.556240	15.867674
25.092015	1323.004955	15.872691
24.995440	1326.739458	15.877709
25.196063	1327.815797	15.882727
25.346735	1324.014322	15.887744
25.054913	1311.535931	15.892762
25.468888	1313.357995	15.897779
25.055056	1316.802258	15.902797
25.066137	1322.853259	15.907815
25.140524	1322.324328	15.912832
25.260198	1322.416361	15.917850
25.297147	1316.872926	15.922867
25.243997	1316.232020	15.927885
25.229997	1314.500559	15.932903
25.279078	1329.182350	15.937920
25.757643	1331.411199	15.942938
25.865476	1333.330699	15.947955
25.503514	1325.344310	15.952973
25.745060	1310.201794	15.957991
25.697277	1312.915591	15.963008
25.357197	1316.761776	15.968026
25.656709	1315.095024	15.973043
25.557536	1320.371845	15.978061
25.817165	1329.998153	15.983079
25.712350	1340.154897	15.988096
25.484124	1338.682816	15.993114
26.109811	1340.866688	15.998131
25.809745	1336.410869	16.003149
25.917998	1334.184865	16.008167
25.941174	1341.692905	16.013184
25.671018	1330.047997	16.018202
25.747578	1342.180961	16.023219
25.700211	1347.612788	16.028237
26.092669	1338.008052	16.033255
26.067090	1345.364726	16.038272
25.646679	1341.864478	16.043290
26.127332	1338.221037	16.048307
25.530171	1339.137917	16.053325
26.015927	1335.737690	16.058343
25.633487	1334.689065	16.063360
25.728483	1340.742739	16.068378
26.256674	1364.938825	16.073395
26.122703	1371.571408	16.078413
26.315111	1374.406916	16.083431
26.628033	1373.642138	16.088448
26.440690	1361.592831	16.093466
26.844968	1337.750682	16.098483
26.572830	1348.569042	16.103501
26.560743	1342.822512	16.108519
26.516189	1334.261895	16.113536
26.372203	1335.169625	16.118554
26.707154	1328.466086	16.123571
26.410518	1331.415270	16.128589
26.414819	1341.677390	16.133607
26.634735	1336.178111	16.138624
26.312551	1336.836985	16.143642
26.289542	1333.918804	16.148659
26.218127	1334.150666	16.153677
26.271132	1337.782906	16.158695
26.775103	1352.572001	16.163712
26.509044	1365.346750	16.168730
26.661602	1375.757989	16.173747
26.643549	1368.203453	16.178765
26.912475	1370.605513	16.183783
27.175638	1369.296284	16.188800
26.484317	1365.786870	16.193818
26.725560	1370.568937	16.198835
26.618693	1372.826041	16.203853
26.709911	1377.426634	16.208871
26.896588	1367.729328	16.213888
26.605883	1369.828258	16.218906
26.980225	1367.733251	16.223923
26.735804	1379.788402	16.228941
26.757357	1371.569937	16.233959
27.015056	1373.434366	16.238976
26.798112	1380.550280	16.243994
26.660037	1369.949695	16.249011
26.461932	1383.939031	16.254029
26.514330	1391.839845	16.259047
26.815440	1398.601891	16.264064
26.739458	1415.963489	16.269082
27.238320	1398.932768	16.274099
27.361643	1395.250149	16.279117
27.484249	1401.749218	16.284135
27.317744	1394.978735	16.289152
27.439599	1399.902766	16.294170
27.813751	1397.620216	16.299187
27.629938	1399.363937	16.304205
27.476665	1397.911349	16.309223
27.374766	1383.547653	16.314240
27.303303	1394.858002	16.319258
27.411902	1400.722668	16.324275
27.519452	1394.138556	16.329293
27.386456	1397.219349	16.334311
27.563969	1389.922600	16.339328
27.776366	1389.754465	16.344346
27.316820	1391.780329	16.349363
27.539853	1397.193667	16.354381
27.636346	1387.900368	16.359399
27.706641	1389.106500	16.364416
27.303792	1397.915889	16.369434
27.568209	1384.976872	16.374451
27.359993	1394.502410	16.379469
27.324398	1402.038299	16.384487
27.617413	1424.258481	16.389504
27.169518	1433.838609	16.394522
27.571539	1425.223826	16.399539
28.104821	1431.025213	16.404557
28.146113	1426.720211	16.409575
28.403558	1430.089588	16.414592
27.712887	1425.587677	16.419610
28.092332	1416.083060	16.424627
28.076979	1427.249731	16.429645
27.698298	1421.776123	16.434663
27.772790	1418.695969	16.439680
27.938888	1422.313673	16.444698
28.317593	1422.545946	16.449715
27.977683	1422.618468	16.454733
27.624179	1424.782498	16.459751
28.536500	1431.719106	16.464768
28.353118	1454.185945	16.469786
28.428171	1434.622839	16.474803
28.109227	1433.079728	16.479821
28.400256	1448.260155	16.484839
28.789692	1440.212127	16.489856
28.415171	1424.283835	16.494874
28.593309	1414.925460	16.499891
28.544183	1419.512452	16.504909
28.530284	1426.401358	16.509927
28.551773	1408.708282	16.514944
28.555902	1413.489197	16.519962
28.718651	1406.546797	16.524979
28.381584	1404.544154	16.529997
28.252076	1425.630204	16.535015
28.427857	1410.269947	16.540032
28.400036	1437.295817	16.545050
28.220514	1434.453080	16.550067
28.640736	1451.388872	16.555085
28.486122	1459.302870	16.560103
28.638913	1450.698358	16.565120
28.402781	1449.075232	16.570138
28.724817	1449.661702	16.575155
28.786517	1446.341762	16.580173
28.904594	1445.346028	16.585191
29.109464	1440.313698	16.590208
28.716413	1444.962058	16.595226
29.021079	1443.311761	16.600243
29.086243	1432.829100	16.605261
28.363372	1443.928082	16.610279
28.907630	1453.203736	16.615296
29.012419	1475.214186	16.620314
29.245025	1471.071427	16.625331
29.458275	1468.657999	16.630349
29.188319	1461.327105	16.635367
29.442866	1453.934340	16.640384
29.171978	1444.027996	16.645402
29.475206	1440.407946	16.650419
29.585062	1444.211892	16.655437
29.465995	1432.884605	16.660455
29.701547	1438.957801	16.665472
29.414561	1439.083969	16.670490
29.357895	1436.747035	16.675507
29.222376	1441.254425	16.680525
29.105902	1438.763618	16.685543
29.415600	1435.869954	16.690560
29.516604	1446.704070	16.695578
29.267328	1437.075023	16.700595
29.398542	1448.879599	16.705613
29.387476	1462.644622	16.710631
29.835486	1466.836527	16.715648
29.667521	1476.313738	16.720666
29.648431	1469.530474	16.725683
29.816253	1465.274227	16.730701
29.853299	1477.293176	16.735719
29.751136	1469.390337	16.740736
29.653799	1478.263835	16.745754
30.035347	1479.299462	16.750771
30.043265	1470.362631	16.755789
29.390228	1476.313429	16.760807
29.611889	1473.919079	16.765824
29.702542	1480.972596	16.770842
29.387753	1470.418661	16.775859
29.794025	1472.919873	16.780877
29.583079	1472.059206	16.785895
29.894458	1464.865282	16.790912
30.211637	1478.717395	16.795930
29.942584	1488.842134	16.800947
29.982535	1481.624562	16.805965
29.980660	1493.907202	16.810983
30.189374	1492.782527	16.816000
29.957459	1497.849290	16.821018
30.419507	1483.166750	16.826035
30.744921	1486.935086	16.831053
30.487656	1489.248946	16.836071
30.525083	1484.897723	16.841088
30.543198	1497.683684	16.846106
30.299572	1485.394993	16.851123
30.718573	1478.662541	16.856141
30.251252	1481.449042	16.861159
30.730905	1467.055299	16.866176
30.556346	1469.929816	16.871194
30.767819	1477.867764	16.876211
30.840662	1455.113522	16.881229
30.560359	1465.690828	16.886247
30.484005	1457.130083	16.891264
30.327689	1444.329234	16.896282
30.549137	1462.200905	16.901299
30.738282	1476.529227	16.906317
30.531836	1473.317363	16.911335
30.633668	1478.749774	16.916352
31.041440	1471.962299	16.921370
30.969248	1471.134403	16.926387
31.291301	1475.530564	16.931405
30.588469	1459.445299	16.936423
30.843265	1460.771123	16.941440
30.850923	1480.146043	16.946458
31.056410	1477.532154	16.951475
30.863072	1474.400199	16.956493
30.641240	1472.961688	16.961511
30.778869	1474.090174	16.966528
30.927215	1475.574909	16.971546
30.909814	1474.846998	16.976563
31.138276	1477.945427	16.981581
30.880284	1467.160289	16.986599
30.986273	1470.124253	16.991616
31.206898	1475.204403	16.996634
31.419466	1496.002951	17.001651
31.064690	1499.445959	17.006669
31.282735	1498.065250	17.011687
31.460246	1512.953717	17.016704
31.753705	1509.942661	17.021722
31.347513	1513.274696	17.026739
31.276825	1508.093026	17.031757
31.427537	1511.416485	17.036775
31.739872	1503.417380	17.041792
31.742296	1517.322526	17.046810
31.563171	1506.534169	17.051827
31.636331	1499.412464	17.056845
31.712661	1509.505138	17.061863
31.780114	1509.275927	17.066880
31.777571	1502.468264	17.071898
31.871403	1500.400897	17.076915
31.862605	1507.218927	17.081933
31.888863	1509.581397	17.086951
31.908544	1503.880141	17.091968
32.003279	1499.007704	17.096986
31.880872	1498.163699	17.102003
31.841978	1493.308229	17.107021
31.997563	1507.755102	17.112039
31.877089	1503.983235	17.117056
32.004879	1498.163737	17.122074
32.003411	1510.148727	17.127091
32.259754	1496.211288	17.132109
31.789763	1502.241084	17.137127
32.010364	1504.646427	17.142144
32.036930	1506.222932	17.147162
31.807772	1505.511905	17.152179
31.874980	1497.199030	17.157197
31.995374	1499.077111	17.162215
32.100304	1502.051491	17.167232
32.270305	1504.068992	17.172250
32.192911	1519.735903	17.177267
32.620754	1541.571624	17.182285
32.385585	1538.321388	17.187303
32.195102	1536.604895	17.192320
32.501010	1525.264390	17.197338
32.313629	1532.246963	17.202355
32.579727	1533.683509	17.207373
32.549884	1539.522293	17.212391
32.870026	1528.472898	17.217408
32.658979	1526.802514	17.222426
32.435882	1533.179657	17.227443
32.744473	1532.610836	17.232461
32.772466	1531.228267	17.237479
32.556593	1525.064029	17.242496
33.175262	1518.456220	17.247514
32.624760	1525.058503	17.252531
32.672818	1522.788884	17.257549
32.689944	1524.788349	17.262567
32.599794	1524.365133	17.267584
32.849959	1527.287372	17.272602
32.610146	1520.703333	17.277619
32.941281	1528.892362	17.282637
32.795781	1551.869941	17.287655
33.072444	1556.921176	17.292672
33.356049	1556.242128	17.297690
32.944569	1561.837927	17.302707
33.184107	1555.655499	17.307725
33.100854	1558.503332	17.312743
33.271808	1557.004038	17.317760
33.293477	1551.322709	17.322778
33.203819	1556.694482	17.327795
33.461688	1556.242294	17.332813
33.537080	1545.262462	17.337831
33.409862	1556.651425	17.342848
33.483469	1550.448591	17.347866
33.791163	1549.806699	17.352883
34.026529	1554.733673	17.357901
33.916538	1554.539098	17.362919
33.679771	1537.911639	17.367936
33.611345	1519.251344	17.372954
33.563690	1523.681058	17.377971
33.783534	1516.867933	17.382989
33.490117	1516.836329	17.388007
33.801165	1531.852136	17.393024
33.801890	1540.355185	17.398042
33.581544	1551.176149	17.403059
33.683186	1555.144647	17.408077
33.713008	1556.414559	17.413095
33.846014	1563.435725	17.418112
34.026486	1544.006022	17.423130
33.760836	1550.243571	17.428147
33.806221	1561.276501	17.433165
33.656135	1556.260473	17.438183
33.775114	1551.350947	17.443200
34.175895	1556.283653	17.448218
33.839599	1554.851256	17.453235
34.226820	1557.835487	17.458253
34.257647	1554.072656	17.463271
33.853115	1570.993514	17.468288
34.233073	1575.249247	17.473306
34.321461	1581.910915	17.478323
34.406047	1572.475595	17.483341
34.244040	1569.409496	17.488359
34.222149	1575.005280	17.493376
34.739961	1570.934246	17.498394
34.588237	1581.322689	17.503411
34.708877	1568.471442	17.508429
34.768580	1569.458306	17.513447
34.298554	1577.284348	17.518464
34.918928	1571.610950	17.523482
34.553187	1578.255548	17.528499
34.647306	1570.650294	17.533517
34.905092	1563.945233	17.538535
34.617367	1571.398281	17.543552
34.933852	1568.447967	17.548570
34.506612	1579.728082	17.553587
34.479620	1570.878249	17.558605
34.662982	1566.376724	17.563623
34.514184	1573.607235	17.568640
34.749074	1566.653038	17.573658
34.829656	1574.931324	17.578675
34.826003	1563.583884	17.583693
35.041058	1569.454248	17.588711
34.540628	1575.324951	17.593728
35.142393	1585.723116	17.598746
35.154217	1592.725546	17.603763
35.105176	1597.819595	17.608781
35.324758	1592.043349	17.613799
34.993938	1607.678026	17.618816
35.505597	1595.222906	17.623834
35.210630	1596.898020	17.628851
35.370240	1602.538418	17.633869
35.576044	1602.642201	17.638887
35.370251	1599.229836	17.643904
35.514572	1601.391928	17.648922
35.479589	1598.268814	17.653939
35.425548	1603.119629	17.658957
35.479732	1600.183524	17.663975
35.186820	1594.595890	17.668992
35.338928	1602.510450	17.674010
35.740309	1599.200084	17.679027
35.709713	1594.374703	17.684045
35.826913	1593.438152	17.689063
35.448788	1595.549982	17.694080
35.433327	1587.417232	17.699098
35.481516	1595.317863	17.704115
35.696711	1603.848489	17.709133
36.146991	1608.614786	17.714151
35.799365	1617.961557	17.719168
35.974912	1612.537613	17.724186
36.391821	1607.401695	17.729203
36.170518	1611.850683	17.734221
36.455111	1611.436985	17.739239
36.166865	1606.913394	17.744256
35.937884	1586.622881	17.749274
36.309000	1608.750514	17.754291
35.887690	1606.893637	17.759309
36.412527	1617.870800	17.764327
35.975261	1615.619367	17.769344
36.294477	1612.364106	17.774362
35.935063	1615.957689	17.779379
35.980045	1621.699112	17.784397
36.039459	1607.489628	17.789415
35.749474	1620.757650	17.794432
36.478680	1630.954495	17.799450
36.534642	1639.205196	17.804467
36.424828	1643.844403	17.809485
36.830704	1641.385732	17.814503
36.395391	1641.439772	17.819520
36.755797	1631.615180	17.824538
36.682451	1639.072199	17.829555
36.768834	1647.018112	17.834573
36.814323	1633.485227	17.839591
36.829142	1647.277039	17.844608
36.919770	1637.783010	17.849626
37.118160	1625.989002	17.854643
36.884378	1631.796177	17.859661
36.916625	1630.349124	17.864679
36.876387	1637.739656	17.869696
36.429111	1643.474649	17.874714
36.806627	1634.527820	17.879731
37.111234	1641.762562	17.884749
37.258856	1645.148758	17.889767
36.910294	1642.508696	17.894784
37.228185	1660.566209	17.899802
37.526360	1652.339673	17.904819
37.404670	1657.743149	17.909837
37.384026	1637.199863	17.914855
37.162216	1648.637985	17.919872
37.280080	1657.863966	17.924890
37.442594	1662.140501	17.929907
37.226787	1665.120677	17.934925
37.622626	1663.992820	17.939943
37.483531	1662.262899	17.944960
37.676432	1656.394397	17.949978
37.637821	1659.722800	17.954995
37.453572	1663.069956	17.960013
37.672552	1659.966074	17.965031
37.715813	1668.315530	17.970048
37.415367	1662.330939	17.975066
37.490290	1663.071625	17.980083
37.287306	1666.407903	17.985101
38.009153	1666.545686	17.990119
37.900212	1663.000388	17.995136
37.860841	1660.939659	18.000154
38.095815	1663.916200	18.005171
38.032649	1669.509982	18.010189
37.683634	1666.119105	18.015207
37.708563	1690.119574	18.020224
38.040586	1681.503030	18.025242
38.316965	1683.966302	18.030259
38.215655	1697.576981	18.035277
38.545241	1684.197866	18.040295
38.139796	1709.029229	18.045312
38.227184	1695.032140	18.050330
38.122611	1692.208856	18.055347
38.339380	1696.125495	18.060365
38.308903	1680.908095	18.065383
38.351520	1690.073705	18.070400
38.601086	1697.108344	18.075418
38.609732	1691.055934	18.080435
38.352328	1691.010702	18.085453
38.858855	1685.708787	18.090471
38.769295	1690.609784	18.095488
38.656200	1688.252219	18.100506
38.974060	1680.676661	18.105523
38.573890	1691.132018	18.110541
39.051956	1683.962213	18.115559
38.672805	1686.661551	18.120576
38.857396	1692.268526	18.125594
39.082999	1682.323874	18.130611
38.702182	1692.652034	18.135629
38.513389	1685.333798	18.140647
38.935232	1695.385048	18.145664
38.991800	1715.161775	18.150682
39.141183	1709.660438	18.155699
39.211023	1711.402626	18.160717
39.411587	1718.177099	18.165735
39.525831	1707.045867	18.170752
39.117619	1706.071149	18.175770
39.584400	1708.024676	18.180787
39.472695	1713.134629	18.185805
39.449525	1707.586029	18.190823
39.554103	1702.324550	18.195840
39.375019	1709.329844	18.200858
39.874230	1707.937886	18.205875
39.531557	1695.090861	18.210893
39.681067	1692.268497	18.215911
39.721478	1698.874569	18.220928
39.519846	1691.861169	18.225946
39.854074	1697.618201	18.230963
39.646429	1703.225242	18.235981
39.694051	1696.990624	18.240999
39.749368	1709.091370	18.246016
39.491748	1716.230693	18.251034
39.740970	1714.533829	18.256051
39.674195	1714.107729	18.261069
39.524106	1705.102199	18.266087
39.753344	1701.136882	18.271104
39.801370	1703.384972	18.276122
39.726706	1693.373804	18.281139
39.794980	1716.314925	18.286157
40.321387	1724.772540	18.291175
40.255116	1731.241157	18.296192
39.998754	1734.876982	18.301210
40.157843	1725.041706	18.306227
40.192222	1737.436842	18.311245
40.233426	1729.120660	18.316263
40.342770	1728.764459	18.321280
40.148440	1733.181272	18.326298
40.404814	1726.713549	18.331315
40.188600	1728.710267	18.336333
40.157816	1726.401094	18.341351
40.516489	1728.626787	18.346368
40.220832	1734.045062	18.351386
40.795102	1740.663117	18.356403
40.509216	1748.507235	18.361421
40.768570	1758.105909	18.366439
41.011294	1741.528308	18.371456
41.124182	1752.396302	18.376474
41.279415	1744.254945	18.381491
41.185196	1739.620521	18.386509
40.953886	1725.240494	18.391527
41.259121	1716.217582	18.396544
40.909325	1720.700825	18.401562
41.074327	1711.638499	18.406579
41.017198	1722.762097	18.411597
41.155910	1714.445358	18.416615
40.893738	1731.190721	18.421632
41.117869	1741.827162	18.426650
41.462392	1736.616954	18.431667
41.145731	1750.244962	18.436685
41.275111	1752.717381	18.441703
41.151577	1753.252510	18.446720
41.619936	1741.017001	18.451738
41.425790	1752.651390	18.456755
41.244418	1744.614076	18.461773
41.387129	1744.436984	18.466791
41.434519	1737.757168	18.471808
41.103284	1737.410789	18.476826
41.460155	1743.805945	18.481843
41.353007	1769.289795	18.486861
41.546873	1766.273694	18.491879
41.981717	1772.432972	18.496896
42.063291	1772.193748	18.501914
41.923569	1774.119570	18.506931
41.977878	1774.028141	18.511949
41.929029	1772.126227	18.516967
42.159411	1773.612787	18.521984
42.010953	1766.758852	18.527002
42.321810	1770.121250	18.532019
42.221898	1771.718880	18.537037
41.921877	1770.502882	18.542055
42.053760	1769.662110	18.547072
42.148362	1765.318680	18.552090
42.258830	1768.526026	18.557107
42.278208	1762.488742	18.562125
42.118628	1769.294408	18.567143
42.400611	1775.562403	18.572160
42.337096	1777.375054	18.577178
42.450941	1763.978575	18.582195
42.176961	1760.639244	18.587213
42.050093	1773.244891	18.592231
42.386542	1787.131693	18.597248
42.572787	1799.970624	18.602266
42.985562	1793.941538	18.607283
42.443112	1800.423329	18.612301
42.536890	1800.839685	18.617319
42.715777	1792.759150	18.622336
42.735996	1798.210081	18.627354
42.830639	1791.252388	18.632371
42.708405	1781.678696	18.637389
42.428300	1785.226932	18.642407
42.358554	1799.990612	18.647424
42.792827	1822.813150	18.652442
43.196264	1819.763588	18.657459
43.143351	1812.213413	18.662477
43.062345	1821.859711	18.667495
43.410055	1808.318064	18.672512
43.338210	1821.634059	18.677530
43.642260	1827.177452	18.682547
43.818370	1804.000166	18.687565
43.683317	1817.198664	18.692583
44.028212	1817.176131	18.697600
43.842450	1813.392932	18.702618
43.691874	1782.781196	18.707635
43.784392	1775.215472	18.712653
43.472862	1775.158515	18.717671
43.943212	1771.404093	18.722688
43.708669	1767.660655	18.727706
43.883077	1758.231044	18.732723
44.091476	1766.225155	18.737741
43.854194	1769.024277	18.742759
43.892918	1763.032215	18.747776
43.681885	1766.265133	18.752794
43.736841	1776.204054	18.757811
44.089049	1790.149270	18.762829
43.892484	1800.181339	18.767847
44.167881	1802.232244	18.772864
43.695561	1815.730342	18.777882
44.115347	1802.432468	18.782899
44.208950	1797.050737	18.787917
43.905419	1804.019953	18.792935
44.249875	1804.185264	18.797952
44.227356	1808.339680	18.802970
44.164126	1803.177935	18.807987
43.967218	1810.696591	18.813005
44.216947	1832.174215	18.818023
44.370008	1822.062741	18.823040
44.415215	1837.518400	18.828058
44.882657	1831.153928	18.833075
44.862797	1831.596739	18.838093
44.577458	1835.730821	18.843111
45.017763	1827.883216	18.848128
45.278586	1823.300319	18.853146
44.989362	1822.151028	18.858163
45.207849	1830.498187	18.863181
44.859683	1822.767889	18.868199
45.236635	1830.976671	18.873216
44.824903	1827.338474	18.878234
44.812922	1822.385747	18.883251
45.028766	1824.047529	18.888269
45.105118	1824.542543	18.893287
45.298320	1823.016519	18.898304
45.027310	1831.764609	18.903322
45.029808	1830.880458	18.908339
45.216992	1827.463922	18.913357
45.128007	1827.021413	18.918375
45.218831	1826.490537	18.923392
44.985550	1834.233890	18.928410
45.295387	1845.850414	18.933427
45.689829	1852.131742	18.938445
45.675955	1869.512128	18.943463
45.320634	1862.569317	18.948480
45.568857	1859.527485	18.953498
45.517974	1862.619995	18.958515
45.449885	1858.438644	18.963533
45.580707	1853.305438	18.968551
45.657882	1845.853815	18.973568
45.489221	1853.489857	18.978586
45.756133	1852.924961	18.983603
46.153124	1871.300321	18.988621
46.101722	1881.562558	18.993639
46.240701	1882.260586	18.998656
46.210657	1888.402257	19.003674
45.988043	1875.673020	19.008691
46.281704	1869.043386	19.013709
46.043761	1888.155504	19.018727
46.249423	1884.506007	19.023744
46.505333	1883.700240	19.028762
46.346483	1892.105653	19.033779
46.578249	1879.857759	19.038797
46.336371	1887.062268	19.043815
46.681075	1880.318105	19.048832
46.609529	1882.489731	19.053850
46.611571	1886.124618	19.058867
46.600640	1873.518258	19.063885
46.859983	1883.945657	19.068903
46.891529	1885.478864	19.073920
47.137119	1885.471953	19.078938
46.470666	1880.700381	19.083955
46.189690	1878.857086	19.088973
46.763792	1882.728110	19.093991
46.861185	1879.265383	19.099008
46.769973	1879.323183	19.104026
46.962454	1903.304761	19.109043
47.210926	1900.367592	19.114061
46.998988	1917.093045	19.119079
47.258357	1905.463924	19.124096
46.993132	1915.811905	19.129114
47.348234	1917.246181	19.134131
47.264534	1906.562035	19.139149
46.981681	1916.654889	19.144167
47.364713	1916.296957	19.149184
47.355208	1917.484628	19.154202
47.247396	1911.902310	19.159219
47.825190	1916.247481	19.164237
47.493042	1924.444569	19.169255
47.768971	1925.698446	19.174272
48.116491	1932.240879	19.179290
47.887170	1930.947050	19.184307
48.142430	1913.580274	19.189325
47.792333	1908.764092	19.194343
47.959408	1902.793871	19.199360
48.104151	1903.216176	19.204378
47.683417	1911.134032	19.209395
47.954186	1909.036978	19.214413
48.036057	1929.252662	19.219431
47.870035	1918.209319	19.224448
48.170721	1922.480022	19.229466
47.997491	1930.015294	19.234483
48.381814	1920.525309	19.239501
48.265660	1930.771707	19.244519
48.230746	1919.241593	19.249536
48.409384	1916.333676	19.254554
48.028620	1924.316972	19.259571
48.307468	1926.575175	19.264589
48.409087	1943.833421	19.269607
48.597285	1948.300850	19.274624
48.567667	1949.009421	19.279642
48.422808	1960.625981	19.284659
48.734515	1949.793600	19.289677
48.666231	1953.243689	19.294695
48.741730	1952.481508	19.299712
48.907239	1955.904773	19.304730
48.516861	1956.116525	19.309747
48.749177	1949.899705	19.314765
48.858397	1965.215598	19.319783
48.866853	1981.791131	19.324800
49.342980	1973.293313	19.329818
49.222394	1976.371776	19.334835
49.508754	1972.994719	19.339853
49.401683	1965.489045	19.344871
49.558908	1975.879844	19.349888
50.253481	1964.288986	19.354906
49.459459	1962.119482	19.359923
49.421393	1943.079485	19.364941
49.207796	1943.327765	19.369959
49.445124	1961.428666	19.374976
49.593344	1961.371712	19.379994
49.569005	1972.269820	19.385011
49.741197	1976.099815	19.390029
49.873881	1979.001402	19.395047
49.491727	1968.185253	19.400064
49.911048	1970.769817	19.405082
49.529456	1965.164618	19.410099
49.786890	1972.108723	19.415117
49.863386	1972.549000	19.420135
49.745367	1971.897922	19.425152
50.326920	1977.899788	19.430170
50.120974	1989.210751	19.435187
50.172805	1990.005066	19.440205
50.467688	2000.201893	19.445223
50.244045	1997.160655	19.450240
50.501798	2002.825726	19.455258
50.246760	2001.880000	19.460275
50.631948	1990.768351	19.465293
50.374480	1994.940581	19.470311
50.673520	2009.210300	19.475328
51.094449	1990.535490	19.480346
50.581096	2006.982341	19.485363
50.522206	2000.665016	19.490381
50.497276	1993.632119	19.495399
50.456967	2000.806718	19.500416
50.302512	1990.741424	19.505434
50.284752	1997.894580	19.510451
50.265370	2020.269009	19.515469
50.771815	2017.058505	19.520487
50.817225	2029.496930	19.525504
50.931897	2018.205578	19.530522
50.730673	2023.956934	19.535539
50.868309	2044.086987	19.540557
51.692365	2043.736875	19.545575
51.637668	2048.458621	19.550592
51.646981	2049.853801	19.555610
51.320279	2048.192235	19.560627
51.637178	2046.096201	19.565645
52.020342	2036.299676	19.570663
51.518196	2043.101250	19.575680
52.146274	2022.177838	19.580698
51.574023	2018.086447	19.585715
51.842223	2013.668793	19.590733
51.688731	2004.695339	19.595751
51.600604	2026.880569	19.600768
52.118083	2027.221011	19.605786
51.875303	2032.749143	19.610803
52.162290	2037.204210	19.615821
52.022689	2036.381911	19.620839
52.198768	2046.771020	19.625856
52.496278	2033.047728	19.630874
52.126370	2030.793171	19.635891
51.983985	2031.476093	19.640909
52.243145	2038.683104	19.645927
52.268044	2035.928509	19.650944
52.252015	2040.299017	19.655962
52.041438	2051.762743	19.660979
52.339716	2038.630990	19.665997
52.550553	2038.160581	19.671015
52.182655	2039.560422	19.676032
52.662606	2033.899434	19.681050
52.416113	2041.383094	19.686067
52.451127	2034.789438	19.691085
52.737908	2049.769413	19.696103
52.669579	2057.275012	19.701120
53.204969	2053.616851	19.706138
52.939652	2056.113601	19.711155
53.336852	2047.234142	19.716173
53.144341	2049.032122	19.721191
52.952195	2052.194268	19.726208
53.307125	2055.503783	19.731226
53.184368	2055.325679	19.736243
52.997268	2050.361860	19.741261
53.073990	2047.110955	19.746279
52.879604	2045.688915	19.751296
53.295522	2051.368808	19.756314
53.279593	2050.960278	19.761331
53.277277	2065.188519	19.766349
53.669967	2075.268062	19.771367
53.253432	2082.068103	19.776384
53.769249	2085.252426	19.781402
53.390835	2077.372682	19.786419
53.560589	2079.796558	19.791437
53.928607	2081.308234	19.796455
53.567843	2091.200319	19.801472
53.979299	2075.879975	19.806490
54.000600	2083.524303	19.811507
53.902996	2077.785332	19.816525
54.306666	2089.899081	19.821543
54.071955	2105.057008	19.826560
54.115625	2104.656540	19.831578
54.310391	2113.540790	19.836595
54.412783	2108.733228	19.841613
54.678803	2099.328424	19.846631
54.453275	2104.718706	19.851648
54.429589	2099.150958	19.856666
54.525770	2101.998764	19.861683
54.445918	2108.453840	19.866701
54.743698	2099.273686	19.871719
54.372919	2107.903195	19.876736
54.814679	2093.581071	19.881754
54.901085	2100.550150	19.886771
54.646561	2096.261957	19.891789
54.881630	2098.172142	19.896807
54.962298	2108.410344	19.901824
54.664815	2097.890316	19.906842
54.777908	2113.247050	19.911859
54.940294	2121.731579	19.916877
55.088814	2132.076092	19.921895
54.767072	2133.262035	19.926912
55.138041	2127.114152	19.931930
55.256008	2130.460282	19.936947
55.311702	2135.137831	19.941965
55.715642	2121.319519	19.946983
55.435497	2136.703664	19.952000
55.621629	2127.238823	19.957018
55.554367	2129.136575	19.962035
55.355609	2136.726752	19.967053
55.649464	2142.910857	19.972071
55.740032	2151.073247	19.977088
56.033333	2150.916538	19.982106
55.851870	2162.458401	19.987123
55.861943	2153.926093	19.992141
56.153655	2153.464952	19.997159
56.341042	2152.790758	20.002176
56.320558	2148.753612	20.007194
56.679593	2153.194051	20.012211
56.264018	2130.763985	20.017229
56.384050	2117.578950	20.022247
56.333490	2120.977136	20.027264
56.388422	2134.308274	20.032282
56.684318	2135.008335	20.037299
56.273969	2127.796767	20.042317
56.503877	2136.412455	20.047335
56.668965	2134.103330	20.052352
56.617338	2139.437134	20.057370
56.368836	2145.966547	20.062387
56.228783	2131.304157	20.067405
56.803424	2139.515277	20.072423
56.710795	2134.532080	20.077440
56.506627	2141.381691	20.082458
56.876199	2150.440994	20.087475
56.972749	2166.932294	20.092493
57.111913	2169.596452	20.097511
56.755746	2168.844969	20.102528
57.125657	2163.349939	20.107546
57.039639	2171.646038	20.112563
56.866529	2166.222040	20.117581
57.358936	2171.545278	20.122599
57.147601	2173.616041	20.127616
57.548937	2190.875427	20.132634
57.794346	2196.112730	20.137651
57.439506	2192.230813	20.142669
57.814687	2195.824977	20.147687
57.675877	2197.148790	20.152704
58.099646	2188.875824	20.157722
58.056996	2195.765889	20.162739
57.756770	2194.977603	20.167757
57.927456	2184.826763	20.172775
57.894223	2205.210241	20.177792
57.761464	2200.237788	20.182810
58.230023	2190.160545	20.187827
58.054197	2197.466083	20.192845
58.150863	2196.710037	20.197863
57.944807	2204.821482	20.202880
58.304379	2217.389230	20.207898
58.335611	2224.826298	20.212915
58.726535	2235.366825	20.217933
58.717148	2229.672466	20.222951
58.739211	2229.460587	20.227968
58.414276	2222.230924	20.232986
58.937748	2219.265771	20.238003
58.827211	2226.574509	20.243021
59.074045	2220.561659	20.248039
58.723397	2214.632583	20.253056
58.845970	2225.842980	20.258074
58.784629	2217.649375	20.263091
58.852860	2223.118505	20.268109
59.274399	2218.389851	20.273127
59.061078	2210.542003	20.278144
59.120291	2219.621533	20.283162
59.387207	2212.860358	20.288179
58.935674	2225.434992	20.293197
59.114436	2235.919643	20.298215
59.120465	2242.929231	20.303232
59.350092	2247.508591	20.308250
59.470191	2244.917147	20.313267
59.245199	2248.688839	20.318285
59.678769	2238.975778	20.323303
59.678807	2251.871248	20.328320
59.567014	2254.700108	20.333338
60.121827	2251.963803	20.338355
59.658882	2265.391458	20.343373
59.989374	2269.688433	20.348391
60.158837	2272.244856	20.353408
60.293067	2274.888393	20.358426
60.728686	2264.149283	20.363443
60.326596	2250.472908	20.368461
60.401913	2243.769756	20.373479
60.203506	2240.608168	20.378496
60.475659	2258.943210	20.383514
60.579568	2260.936697	20.388531
60.560343	2278.925853	20.393549
60.763372	2256.951598	20.398567
60.656142	2268.502728	20.403584
60.746891	2274.958814	20.408602
60.748479	2256.466157	20.413619
60.652383	2268.381162	20.418637
60.913409	2277.089022	20.423655
61.035559	2273.304823	20.428672
60.945190	2277.658945	20.433690
60.938571	2272.717194	20.438707
60.907521	2274.955209	20.443725
61.187562	2271.925754	20.448743
60.919289	2269.947449	20.453760
60.989060	2273.402156	20.458778
61.357921	2274.459227	20.463795
61.227413	2287.931368	20.468813
61.567940	2299.526630	20.473831
61.393400	2295.304094	20.478848
61.309315	2296.679891	20.483866
61.469017	2291.048504	20.488883
61.333008	2292.271675	20.493901
61.186377	2289.484557	20.498919
61.857012	2297.479525	20.503936
61.546796	2313.253228	20.508954
61.862098	2314.882292	20.513971
61.935325	2317.729404	20.518989
62.104094	2321.657877	20.524007
62.294763	2311.712098	20.529024
62.234396	2314.010076	20.534042
62.250274	2311.522450	20.539059
62.103270	2307.702215	20.544077
62.235402	2320.071628	20.549095
62.499037	2320.042841	20.554112
62.673077	2333.538311	20.559130
62.544334	2344.971804	20.564147
62.567663	2339.492648	20.569165
62.603625	2338.328553	20.574183
62.888669	2343.997902	20.579200
62.738692	2344.522854	20.584218
62.732379	2349.489234	20.589235
62.943801	2348.949238	20.594253
62.709599	2330.288978	20.599271
62.883115	2338.514723	20.604288
62.849975	2346.470907	20.609306
63.053734	2358.818477	20.614323
62.867627	2365.577611	20.619341
63.107335	2369.571336	20.624359
63.255863	2360.449546	20.629376
63.322108	2364.143615	20.634394
63.669527	2367.696742	20.639411
63.653663	2361.762086	20.644429
63.768140	2364.502399	20.649447
63.411962	2360.713566	20.654464
63.572609	2360.355370	20.659482
64.034922	2364.553234	20.664499
63.979032	2365.171094	20.669517
64.069509	2369.968153	20.674535
64.212577	2363.215766	20.679552
64.130105	2370.760662	20.684570
64.068326	2366.581279	20.689587
64.016306	2371.069236	20.694605
64.384578	2385.314283	20.699623
64.523465	2384.897680	20.704640
64.307700	2390.476392	20.709658
64.537624	2383.287630	20.714675
64.721145	2388.485230	20.719693
64.744352	2386.700259	20.724711
64.945616	2380.971429	20.729728
64.643089	2386.683364	20.734746
64.657418	2376.809987	20.739763
64.551925	2376.790626	20.744781
64.667789	2382.375553	20.749799
64.957838	2377.436120	20.754816
64.546214	2386.804951	20.759834
64.803446	2377.335295	20.764851
64.903747	2409.852655	20.769869
64.911644	2415.467245	20.774887
64.945912	2410.009680	20.779904
65.126327	2422.626294	20.784922
65.314662	2413.189456	20.789939
65.426245	2419.676999	20.794957
65.133138	2423.082067	20.799975
65.377973	2426.493117	20.804992
65.512888	2448.690910	20.810010
65.787503	2442.405294	20.815027
65.829269	2439.627960	20.820045
65.641106	2444.870660	20.825063
65.983167	2433.252871	20.830080
65.721305	2437.186397	20.835098
65.919709	2438.345066	20.840115
66.369422	2434.994456	20.845133
66.057485	2436.769304	20.850151
66.563795	2454.257682	20.855168
66.134145	2465.402825	20.860186
66.387214	2461.606395	20.865203
66.796691	2463.053194	20.870221
66.584744	2469.066111	20.875239
66.946524	2452.624756	20.880256
66.840160	2463.816862	20.885274
66.707611	2466.333270	20.890291
66.926791	2454.046060	20.895309
66.942489	2454.863495	20.900327
67.003523	2449.221390	20.905344
66.710439	2466.310818	20.910362
67.052184	2455.813645	20.915379
67.382274	2457.868594	20.920397
66.835604	2469.351752	20.925415
67.266312	2450.918651	20.930432
67.283113	2455.809007	20.935450
67.143872	2456.657754	20.940467
66.970491	2461.839557	20.945485
66.970994	2488.711421	20.950503
67.290933	2482.531873	20.955520
67.289997	2481.106563	20.960538
67.423810	2488.221515	20.965555
67.547373	2500.175591	20.970573
67.584049	2514.365521	20.975591
67.900807	2508.220148	20.980608
68.059716	2511.458422	20.985626
67.691559	2521.977348	20.990643
68.026601	2519.244837	20.995661
67.713252	2527.781827	21.000679
67.908868	2520.403213	21.005696
68.300919	2527.195611	21.010714
68.172530	2547.661598	21.015731
68.535634	2544.220166	21.020749
68.403136	2542.668372	21.025767
68.634324	2536.125347	21.030784
68.837644	2545.478674	21.035802
68.785219	2537.654659	21.040819
69.227167	2536.026443	21.045837
68.652567	2539.874873	21.050855
68.693639	2540.542657	21.055872
68.929254	2538.943026	21.060890
69.289301	2536.944121	21.065907
69.206468	2541.361831	21.070925
68.948062	2539.253523	21.075943
69.009284	2540.029781	21.080960
69.194373	2531.051052	21.085978
69.105699	2540.648872	21.090995
69.293672	2557.139654	21.096013
69.149377	2561.174445	21.101031
69.584783	2566.908196	21.106048
69.445110	2564.737158	21.111066
69.468567	2570.074253	21.116083
69.456748	2565.830068	21.121101
69.828291	2580.722937	21.126119
70.153977	2588.660500	21.131136
70.403376	2584.689068	21.136154
70.385015	2583.016448	21.141171
70.633712	2578.194210	21.146189
70.461389	2559.268544	21.151207
70.518761	2561.890385	21.156224
70.061535	2563.580012	21.161242
70.331962	2571.149559	21.166259
70.633451	2579.050370	21.171277
70.589831	2588.682111	21.176295
70.720384	2579.516513	21.181312
70.991339	2588.363056	21.186330
70.627138	2583.463563	21.191347
70.917188	2577.900488	21.196365
70.839976	2588.959727	21.201383
70.768705	2577.455403	21.206400
70.788611	2590.408104	21.211418
70.684887	2592.967798	21.216435
71.077744	2591.846867	21.221453
71.081725	2611.534425	21.226471
70.945521	2610.329669	21.231488
71.342220	2615.355121	21.236506
71.299278	2614.065471	21.241523
71.395708	2603.624876	21.246541
71.543736	2627.184444	21.251559
71.322383	2633.238938	21.256576
71.887209	2644.589734	21.261594
71.469447	2653.341670	21.266611
71.842665	2641.765227	21.271629
71.397270	2654.885613	21.276647
71.805975	2647.467397	21.281664
72.104953	2671.144796	21.286682
72.268504	2675.655090	21.291699
72.441502	2675.265714	21.296717
72.608517	2682.186699	21.301735
72.605066	2663.827450	21.306752
72.577469	2667.691617	21.311770
72.815202	2667.037624	21.316787
72.975984	2656.915275	21.321805
72.648326	2661.905921	21.326823
72.692625	2662.474365	21.331840
72.857782	2663.275578	21.336858
72.547041	2662.582305	21.341875
72.891311	2653.541967	21.346893
72.951831	2655.223406	21.351911
73.252904	2667.751389	21.356928
72.967174	2655.809838	21.361946
72.882139	2658.615650	21.366963
73.392886	2662.711111	21.371981
73.302046	2668.248021	21.376999
73.432717	2678.216348	21.382016
73.498535	2672.988698	21.387034
72.907338	2681.375831	21.392051
73.334191	2674.072509	21.397069
73.623907	2675.085409	21.402087
73.718904	2678.785037	21.407104
73.762409	2697.950853	21.412122
73.795052	2710.914149	21.417139
74.135237	2701.524086	21.422157
74.328740	2711.079911	21.427175
74.224314	2706.722849	21.432192
74.049494	2709.766327	21.437210
74.180884	2708.113828	21.442227
74.169720	2699.844750	21.447245
74.161233	2714.806846	21.452263
74.445634	2719.247186	21.457280
74.605728	2723.573037	21.462298
74.543002	2735.181724	21.467315
74.804561	2725.401908	21.472333
74.731079	2733.520853	21.477351
74.877454	2734.856637	21.482368
75.187487	2723.759443	21.487386
75.422352	2740.224170	21.492403
75.082462	2725.762533	21.497421
74.989205	2721.556761	21.502439
75.072784	2742.718249	21.507456
75.582181	2739.612422	21.512474
75.297026	2759.985703	21.517491
75.775068	2739.442398	21.522509
75.546340	2757.937962	21.527527
75.713372	2762.125678	21.532544
75.955164	2745.116473	21.537562
75.750205	2746.588656	21.542579
75.727588	2741.310246	21.547597
75.943626	2755.662086	21.552615
75.833236	2739.914162	21.557632
76.369541	2760.990236	21.562650
76.386682	2773.825051	21.567667
76.395197	2771.802320	21.572685
76.401250	2778.298398	21.577703
76.066687	2783.689019	21.582720
76.272566	2774.019549	21.587738
76.137276	2781.475150	21.592755
76.550173	2775.063800	21.597773
76.723566	2786.688623	21.602791
76.529090	2801.797278	21.607808
76.889850	2807.519835	21.612826
76.772787	2813.528426	21.617843
77.239162	2802.530137	21.622861
77.353742	2804.488076	21.627879
77.372306	2803.039239	21.632896
77.305836	2794.309197	21.637914
77.052553	2806.760797	21.642931
77.038616	2792.639308	21.647949
77.432074	2819.353708	21.652967
77.591691	2823.927684	21.657984
77.691457	2821.043458	21.663002
77.544202	2826.838945	21.668019
77.793743	2823.626049	21.673037
77.817236	2822.208284	21.678055
77.818314	2827.465903	21.683072
78.234766	2819.503245	21.688090
78.407500	2818.565515	21.693107
78.765323	2817.092898	21.698125
78.574601	2809.276637	21.703143
78.487396	2816.164498	21.708160
78.824332	2812.986767	21.713178
78.561619	2811.158447	21.718195
78.694763	2807.970693	21.723213
78.551112	2808.943409	21.728231
78.240212	2813.102639	21.733248
78.960256	2810.329292	21.738266
78.861828	2810.761494	21.743283
78.713276	2806.712859	21.748301
78.935721	2830.193515	21.753319
78.500847	2835.643641	21.758336
79.078472	2843.916456	21.763354
79.055521	2848.398173	21.768371
79.016104	2838.412523	21.773389
78.964240	2848.084565	21.778407
79.246804	2868.724394	21.783424
79.211108	2875.123480	21.788442
79.323843	2872.059945	21.793459
79.492628	2876.629273	21.798477
79.693698	2879.997265	21.803495
79.403759	2890.375175	21.808512
79.801930	2894.476704	21.813530
79.779318	2907.222534	21.818547
79.762412	2901.108915	21.823565
79.995056	2912.810259	21.828583
80.166847	2925.114551	21.833600
80.384317	2922.304947	21.838618
80.350414	2932.211070	21.843635
80.844133	2924.159217	21.848653
80.935443	2921.643674	21.853671
80.608704	2921.548279	21.858688
80.999064	2931.425631	21.863706
81.086834	2925.816334	21.868723
80.684973	2923.366931	21.873741
80.928359	2927.571995	21.878759
80.687026	2933.239374	21.883776
81.167031	2938.308841	21.888794
81.249826	2945.822180	21.893811
81.400292	2954.531765	21.898829
81.473123	2952.885373	21.903847
81.486282	2955.955314	21.908864
81.967719	2947.050007	21.913882
81.973167	2952.866763	21.918899
81.851773	2957.932862	21.923917
81.997973	2942.946625	21.928935
81.962295	2945.645912	21.933952
82.274284	2942.457710	21.938970
81.855190	2946.166373	21.943987
82.200658	2949.382179	21.949005
82.146046	2945.661276	21.954023
82.227006	2976.222682	21.959040
82.371307	2966.986870	21.964058
82.547217	2980.234577	21.969075
82.434045	2975.236393	21.974093
82.769714	2968.086186	21.979111
82.494094	2970.963702	21.984128
82.632128	2972.977233	21.989146
82.420250	2983.325377	21.994163
82.662527	2999.905293	21.999181
83.178495	2999.006894	22.004199
82.976999	3012.613437	22.009216
83.194275	3004.518250	22.014234
83.107549	3006.526801	22.019251
83.371423	3007.142043	22.024269
83.752899	2996.339529	22.029287
83.447145	3001.305404	22.034304
83.326697	2993.765220	22.039322
83.703520	3014.588873	22.044339
83.735881	3032.291259	22.049357
84.160948	3021.509869	22.054375
83.900192	3023.087750	22.059392
84.543775	3018.265673	22.064410
84.358243	3022.363693	22.069427
84.480339	3019.644237	22.074445
84.492975	3008.188127	22.079463
84.497699	3024.836849	22.084480
84.290373	3008.654688	22.089498
84.141008	3016.361141	22.094515
84.081702	3018.476576	22.099533
84.856926	3017.510928	22.104551
84.490336	3026.718180	22.109568
84.815959	3027.934217	22.114586
84.906499	3035.842761	22.119603
84.805924	3059.313365	22.124621
85.043450	3050.541213	22.129639
85.184842	3059.121653	22.134656
85.489492	3055.889367	22.139674
85.393433	3058.951000	22.144691
84.953420	3055.883888	22.149709
85.184983	3060.297234	22.154727
85.342496	3074.134258	22.159744
85.550206	3072.878542	22.164762
85.616344	3079.619926	22.169779
85.522272	3083.182397	22.174797
85.853127	3088.920236	22.179815
85.685613	3108.006866	22.184832
86.048862	3099.772553	22.189850
86.162884	3106.734374	22.194867
85.834406	3119.791935	22.199885
86.549251	3106.751266	22.204903
86.343086	3132.214159	22.209920
86.778941	3129.513307	22.214938
86.911748	3122.218211	22.219955
86.329939	3136.578625	22.224973
86.733361	3121.578450	22.229991
86.462444	3133.438365	22.235008
86.732449	3135.624591	22.240026
87.082181	3145.002513	22.245043
87.110773	3162.032465	22.250061
87.169464	3157.716823	22.255079
87.102138	3163.363012	22.260096
87.149598	3171.915336	22.265114
87.643956	3167.233616	22.270131
87.860229	3174.232507	22.275149
88.066351	3184.802649	22.280167
88.140839	3174.106250	22.285184
88.175506	3170.762653	22.290202
88.228925	3155.123847	22.295219
87.694110	3155.726589	22.300237
88.312271	3165.027885	22.305255
88.482892	3174.011419	22.310272
88.392552	3175.585957	22.315290
88.407709	3172.119998	22.320307
88.452878	3186.696136	22.325325
88.766117	3175.087871	22.330343
88.673954	3176.393034	22.335360
88.912735	3173.866468	22.340378
88.765742	3166.483731	22.345395
88.619537	3165.887650	22.350413
88.735724	3170.051203	22.355431
88.482961	3190.945664	22.360448
88.388366	3206.629528	22.365466
89.163094	3210.754744	22.370483
89.119886	3213.691142	22.375501
88.998698	3213.968458	22.380519
89.187654	3243.847212	22.385536
89.365552	3242.443657	22.390554
89.499543	3229.686657	22.395571
89.504006	3240.028356	22.400589
90.107164	3247.334600	22.405607
90.176079	3261.043916	22.410624
90.371799	3258.172887	22.415642
90.424499	3255.434543	22.420659
90.134564	3257.481036	22.425677
90.761876	3258.995263	22.430695
90.831689	3265.119207	22.435712
90.750958	3248.145031	22.440730
90.785947	3248.303236	22.445747
90.571794	3258.251556	22.450765
90.848414	3252.020007	22.455783
90.709891	3248.558953	22.460800
90.926665	3254.644436	22.465818
91.291265	3252.359659	22.470835
90.984412	3246.681993	22.475853
91.008466	3256.227575	22.480871
90.800956	3258.663586	22.485888
90.508237	3273.224775	22.490906
90.778053	3273.633146	22.495923
90.780569	3296.500081	22.500941
91.189908	3310.533888	22.505959
91.482269	3308.701580	22.510976
91.530735	3326.264242	22.515994
91.761838	3332.664705	22.521011
92.298490	3338.611540	22.526029
92.367295	3337.805124	22.531047
92.790961	3329.499291	22.536064
92.543375	3336.794978	22.541082
92.802986	3326.178117	22.546099
92.752875	3333.666363	22.551117
92.841390	3322.786052	22.556135
93.050345	3324.763501	22.561152
92.811591	3328.574340	22.566170
93.252045	3317.334309	22.571187
93.106426	3324.461963	22.576205
92.808835	3332.674552	22.581223
93.206066	3324.204983	22.586240
93.168405	3322.085482	22.591258
93.134688	3328.674581	22.596275
93.108020	3350.436207	22.601293
93.407554	3354.338415	22.606311
93.551057	3349.836662	22.611328
93.369375	3362.289473	22.616346
93.612468	3355.155567	22.621363
93.834284	3381.377264	22.626381
93.998420	3395.405998	22.631399
94.150385	3382.551416	22.636416
94.227679	3389.632424	22.641434
94.474017	3388.275420	22.646451
94.546715	3389.711623	22.651469
94.367285	3391.250512	22.656487
94.502875	3381.343071	22.661504
94.220341	3383.654493	22.666522
95.004683	3393.681604	22.671539
94.802509	3417.392761	22.676557
94.460056	3413.137429	22.681575
94.886180	3404.146909	22.686592
94.969255	3424.172818	22.691610
94.977760	3411.155307	22.696627
94.976014	3414.148276	22.701645
95.143609	3439.535345	22.706663
95.425645	3436.759861	22.711680
95.818109	3447.651749	22.716698
95.813681	3441.781521	22.721715
95.689254	3440.096807	22.726733
95.640400	3440.253515	22.731751
95.867773	3435.715831	22.736768
95.589906	3444.360646	22.741786
95.839260	3458.546612	22.746803
95.940106	3468.883955	22.751821
96.376240	3477.768281	22.756839
96.474559	3463.847708	22.761856
96.354255	3484.163596	22.766874
96.512546	3464.919399	22.771891
96.771286	3481.324671	22.776909
96.676065	3492.204658	22.781927
97.162501	3489.034764	22.786944
96.678621	3493.335748	22.791962
96.926617	3482.930147	22.796979
97.203997	3492.639917	22.801997
97.039335	3498.610181	22.807015
97.311399	3505.362998	22.812032
97.261273	3514.148170	22.817050
97.385751	3511.345559	22.822067
97.588735	3516.791700	22.827085
97.612265	3505.907038	22.832103
97.801542	3515.523901	22.837120
97.692507	3525.308567	22.842138
98.202236	3522.761190	22.847155
98.000982	3538.687026	22.852173
98.072774	3536.071856	22.857191
98.169776	3541.224890	22.862208
98.179212	3548.821116	22.867226
98.670124	3562.974350	22.872243
98.869598	3570.709656	22.877261
99.002036	3577.872582	22.882279
98.857581	3565.193600	22.887296
98.721160	3565.240370	22.892314
99.102842	3563.752326	22.897331
99.023112	3574.939651	22.902349
99.043601	3565.469614	22.907367
99.638934	3587.078398	22.912384
99.667756	3591.475003	22.917402
99.788155	3595.812777	22.922419
99.854830	3597.760229	22.927437
100.051338	3596.105144	22.932455
100.189153	3596.079827	22.937472
99.966048	3591.325986	22.942490
99.996413	3596.418004	22.947507
100.248146	3597.273859	22.952525
100.030475	3592.425813	22.957543
100.289368	3592.967100	22.962560
99.912912	3601.112940	22.967578
100.116424	3615.660955	22.972595
100.268029	3616.606191	22.977613
100.331747	3619.681295	22.982631
100.649756	3637.427329	22.987648
100.740376	3650.335767	22.992666
101.081634	3664.297681	22.997683
101.076089	3651.180716	23.002701
101.070907	3653.794772	23.007719
101.214228	3653.726420	23.012736
101.658397	3668.651253	23.017754
101.683472	3674.896926	23.022771
101.838821	3681.504145	23.027789
101.840762	3678.910729	23.032807
102.075018	3675.926563	23.037824
102.118675	3675.243971	23.042842
102.187101	3678.051773	23.047859
102.572966	3675.344131	23.052877
102.199008	3675.867946	23.057895
102.231274	3680.315189	23.062912
102.177386	3674.848715	23.067930
102.473215	3664.598474	23.072947
102.350514	3666.197700	23.077965
102.354386	3679.191363	23.082983
102.699029	3694.094478	23.088000
102.239218	3700.366739	23.093018
102.430392	3694.031811	23.098035
102.686008	3715.662657	23.103053
102.678630	3726.231441	23.108071
103.114199	3728.976618	23.113088
103.281965	3731.295179	23.118106
103.532612	3753.913518	23.123123
103.816213	3755.173173	23.128141
103.465422	3759.054204	23.133159
104.018065	3752.639443	23.138176
103.760088	3753.470082	23.143194
104.002624	3752.468796	23.148211
104.220802	3759.646379	23.153229
103.856497	3782.405350	23.158247
104.230275	3785.409174	23.163264
104.407975	3794.065125	23.168282
104.154646	3787.535102	23.173299
104.407476	3795.675880	23.178317
104.563974	3805.492829	23.183335
105.010816	3808.083795	23.188352
105.025295	3818.093512	23.193370
105.361256	3805.779837	23.198387
105.566665	3807.408326	23.203405
105.488944	3814.269470	23.208423
105.899064	3799.402972	23.213440
105.929976	3799.997294	23.218458
105.593837	3791.888026	23.223475
105.768119	3802.691807	23.228493
105.622667	3823.116231	23.233511
106.085446	3828.217976	23.238528
106.277264	3833.681428	23.243546
106.194378	3843.100551	23.248563
106.334294	3842.931973	23.253581
106.112825	3833.291515	23.258599
106.412071	3832.558808	23.263616
106.587730	3843.673023	23.268634
106.395123	3850.633089	23.273651
106.748824	3860.122997	23.278669
106.823203	3863.809387	23.283687
107.029068	3859.482224	23.288704
106.864415	3864.786478	23.293722
107.210315	3866.466956	23.298739
107.379369	3872.107020	23.303757
107.234778	3881.330848	23.308775
107.576039	3886.370014	23.313792
107.448974	3895.851982	23.318810
107.751934	3890.930805	23.323827
107.792212	3902.393028	23.328845
107.647577	3909.607402	23.333863
107.994956	3913.358538	23.338880
108.211927	3920.776163	23.343898
108.275523	3922.127305	23.348915
108.543606	3915.465793	23.353933
108.293841	3935.606416	23.358951
108.733915	3941.283219	23.363968
108.929662	3948.140969	23.368986
108.752819	3938.554489	23.374003
108.778542	3940.946554	23.379021
108.903881	3947.066318	23.384039
108.873193	3952.571303	23.389056
108.866812	3964.661371	23.394074
109.079083	3964.198547	23.399091
109.427096	3972.101639	23.404109
109.451120	3979.303531	23.409127
109.783121	3969.969572	23.414144
109.887801	3971.319442	23.419162
109.566786	3970.447877	23.424179
109.544469	3978.751935	23.429197
109.898498	4003.079179	23.434215
110.090393	3999.174373	23.439232
110.370634	4004.422877	23.444250
110.289206	4002.693594	23.449267
110.272982	4016.449143	23.454285
110.372151	4019.446026	23.459303
110.802939	4013.982418	23.464320
110.805889	4025.502081	23.469338
110.934373	4022.070357	23.474355
111.448277	4023.312059	23.479373
111.253281	4043.619759	23.484391
111.486817	4049.726803	23.489408
111.632862	4038.363246	23.494426
111.250609	4045.358673	23.499443
111.685690	4042.492439	23.504461
111.653750	4042.231780	23.509479
111.662595	4042.106906	23.514496
111.833168	4059.497855	23.519514
112.050311	4077.515789	23.524531
112.175062	4060.907569	23.529549
112.053067	4075.152705	23.534567
112.497405	4080.130019	23.539584
112.860425	4081.106494	23.544602
112.539311	4105.115524	23.549619
112.716815	4102.431215	23.554637
112.774949	4102.482452	23.559655
113.151276	4111.551048	23.564672
113.276065	4106.856888	23.569690
113.254612	4110.020181	23.574707
113.355267	4111.247103	23.579725
113.361163	4129.315752	23.584743
113.463153	4131.553508	23.589760
113.736784	4128.949376	23.594778
113.348904	4135.525682	23.599795
113.513957	4151.706193	23.604813
113.342550	4162.286234	23.609831
113.810983	4167.632835	23.614848
114.345879	4166.291079	23.619866
114.266310	4185.044409	23.624883
115.026782	4181.260969	23.629901
114.991946	4184.432000	23.634919
115.303780	4182.684961	23.639936
115.363929	4183.994962	23.644954
115.159141	4175.240147	23.649971
115.088109	4169.725542	23.654989
115.412503	4176.881436	23.660007
115.496756	4177.423650	23.665024
115.603709	4175.654952	23.670042
115.609748	4183.292602	23.675059
115.366615	4180.760070	23.680077
115.483629	4181.144897	23.685095
115.544612	4196.674126	23.690112
116.025685	4210.490592	23.695130
115.764463	4219.243717	23.700147
116.002001	4206.526683	23.705165
116.044802	4216.565050	23.710183
116.226417	4233.035439	23.715200
116.628029	4234.290596	23.720218
116.633092	4243.566684	23.725235
116.514018	4227.841912	23.730253
116.777522	4246.654380	23.735271
116.714974	4245.044789	23.740288
116.764754	4259.990084	23.745306
116.659134	4279.586840	23.750323
116.904985	4263.216277	23.755341
117.133390	4281.258573	23.760359
117.279544	4290.168055	23.765376
117.862285	4292.487032	23.770394
117.756154	4296.894718	23.775411
118.095752	4290.919684	23.780429
117.914975	4290.630069	23.785447
117.970667	4302.365640	23.790464
118.820091	4313.233816	23.795482
118.787654	4321.546816	23.800499
119.245029	4312.065554	23.805517
119.031696	4313.536508	23.810535
119.184010	4321.254390	23.815552
119.373385	4304.743110	23.820570
119.248911	4316.831310	23.825587
119.495266	4311.832738	23.830605
119.404479	4307.995039	23.835623
119.030200	4318.364997	23.840640
119.527831	4308.385333	23.845658
119.185878	4307.446732	23.850675
119.433305	4302.420426	23.855693
119.685100	4309.770276	23.860711
119.596530	4319.492213	23.865728
119.890208	4322.283780	23.870746
119.866613	4333.639546	23.875763
120.114089	4347.853804	23.880781
120.160870	4361.599640	23.885799
120.176886	4365.454463	23.890816
120.646489	4355.966036	23.895834
120.598509	4379.688220	23.900851
120.467865	4389.790792	23.905869
121.001139	4389.659972	23.910887
120.848692	4392.731970	23.915904
121.057009	4398.921670	23.920922
121.127176	4413.627905	23.925939
121.068014	4414.066653	23.930957
121.517005	4428.631170	23.935975
121.551910	4444.568518	23.940992
121.991165	4435.257114	23.946010
121.930228	4446.846703	23.951027
122.108655	4444.214548	23.956045
122.168271	4437.875071	23.961063
122.336432	4466.600896	23.966080
122.422199	4467.727151	23.971098
122.283946	4472.275635	23.976115
122.858813	4475.696786	23.981133
122.852809	4472.691143	23.986151
122.966340	4490.492807	23.991168
123.040549	4489.179114	23.996186
122.893616	4502.727544	24.001203
122.977396	4505.748325	24.006221
123.362238	4502.428475	24.011239
123.284266	4527.377164	24.016256
123.555168	4531.165106	24.021274
123.696890	4543.605974	24.026291
123.736707	4528.956674	24.031309
124.144231	4544.586477	24.036327
123.947166	4562.740743	24.041344
124.024214	4565.107493	24.046362
124.175746	4573.857185	24.051379
124.335622	4569.008262	24.056397
124.712533	4584.892391	24.061415
124.412111	4605.930488	24.066432
124.496256	4603.769818	24.071450
124.733895	4613.425831	24.076467
124.778329	4616.523218	24.081485
124.904027	4636.802322	24.086503
124.975183	4634.848925	24.091520
125.724306	4632.850436	24.096538
125.713950	4642.982905	24.101555
125.689426	4651.275874	24.106573
126.232907	4662.363364	24.111591
126.328927	4660.249940	24.116608
126.542341	4646.435678	24.121626
126.415143	4654.341652	24.126643
126.580545	4658.202574	24.131661
126.821244	4659.554440	24.136679
126.117544	4662.853412	24.141696
126.286342	4659.492845	24.146714
126.533717	4683.134008	24.151731
126.473732	4680.189216	24.156749
127.203081	4692.199227	24.161767
127.057358	4705.985443	24.166784
127.533960	4713.218411	24.171802
127.540142	4720.001125	24.176819
127.289122	4714.547172	24.181837
127.781644	4726.871951	24.186855
127.806993	4739.732231	24.191872
127.870715	4744.255295	24.196890
127.770490	4742.738498	24.201907
128.012074	4763.982151	24.206925
128.589181	4771.222163	24.211943
128.497018	4776.964384	24.216960
128.483754	4778.733054	24.221978
128.184620	4785.358750	24.226995
128.599090	4794.789974	24.232013
129.269194	4799.047885	24.237031
129.037480	4799.616344	24.242048
129.141642	4806.717181	24.247066
129.610885	4817.447337	24.252083
129.420065	4823.736625	24.257101
129.551131	4820.244059	24.262119
129.699318	4828.164858	24.267136
130.015160	4836.669028	24.272154
130.280114	4842.782612	24.277171
130.170379	4852.638702	24.282189
130.775173	4844.599014	24.287207
130.377761	4850.073960	24.292224
130.122317	4847.804396	24.297242
130.694621	4872.071733	24.302259
130.929582	4877.656782	24.307277
131.351891	4871.709990	24.312295
130.987310	4879.478517	24.317312
131.300836	4885.589210	24.322330
131.596776	4904.937314	24.327347
131.649225	4912.335743	24.332365
131.974407	4907.173552	24.337383
131.886943	4913.773776	24.342400
131.819739	4904.045347	24.347418
131.948290	4915.221660	24.352435
131.740618	4927.085476	24.357453
131.975097	4941.864674	24.362471
132.058361	4939.287928	24.367488
132.250481	4962.377969	24.372506
132.367291	4969.474034	24.377523
132.469683	4977.344597	24.382541
132.727698	4985.517824	24.387559
132.665476	5008.626335	24.392576
132.867683	5010.047196	24.397594
132.964561	5013.502957	24.402611
133.338167	5038.735750	24.407629
133.604408	5023.591446	24.412647
134.043850	5039.425152	24.417664
133.838642	5038.134353	24.422682
134.109505	5024.290186	24.427699
134.203773	5037.766937	24.432717
134.942380	5034.044792	24.437735
134.709634	5061.546111	24.442752
134.765928	5052.743724	24.447770
134.820653	5051.268229	24.452787
134.684394	5054.057735	24.457805
134.944576	5044.425923	24.462823
134.906587	5056.516547	24.467840
135.024935	5054.582074	24.472858
135.502771	5064.449488	24.477875
135.490627	5081.759555	24.482893
135.516145	5076.486573	24.487911
135.631563	5083.780576	24.492928
135.787583	5096.603022	24.497946
135.900032	5106.958436	24.502963
135.765702	5109.538165	24.507981
135.949655	5109.089833	24.512999
136.349143	5134.865799	24.518016
136.510909	5131.320056	24.523034
136.941808	5127.066789	24.528051
136.565464	5137.314782	24.533069
137.217435	5149.459205	24.538087
137.230024	5159.146837	24.543104
137.383948	5160.300861	24.548122
137.542029	5162.179858	24.553139
137.582600	5167.144706	24.558157
138.065106	5158.932134	24.563175
138.110871	5166.882628	24.568192
138.188535	5169.444269	24.573210
138.509735	5189.490194	24.578227
138.378527	5194.678335	24.583245
138.502049	5189.218239	24.588263
138.677168	5191.144823	24.593280
138.885894	5183.338141	24.598298
138.837631	5187.369945	24.603315
138.858875	5188.095457	24.608333
139.239727	5205.401360	24.613351
139.202036	5216.560865	24.618368
139.161853	5223.035679	24.623386
139.589682	5226.636429	24.628403
139.702586	5218.906592	24.633421
139.471724	5229.335350	24.638439
139.708495	5239.541950	24.643456
139.520939	5239.111689	24.648474
140.330109	5255.583020	24.653491
140.075610	5266.385824	24.658509
140.269677	5267.862391	24.663527
140.522121	5274.597174	24.668544
140.654903	5285.278514	24.673562
140.695058	5295.345967	24.678579
140.819048	5297.958248	24.683597
140.875437	5302.902807	24.688615
140.817982	5317.028557	24.693632
141.312795	5327.060673	24.698650
141.609010	5323.351712	24.703667
141.541533	5336.379018	24.708685
141.915868	5348.083987	24.713703
142.155130	5351.008369	24.718720
142.648088	5350.445973	24.723738
142.654114	5350.124289	24.728755
142.644404	5349.378387	24.733773
142.815432	5343.941100	24.738791
143.126599	5337.855395	24.743808
143.078981	5338.033178	24.748826
143.370281	5339.860654	24.753843
143.111996	5345.536428	24.758861
143.412946	5358.124883	24.763879
143.593969	5370.751277	24.768896
143.275311	5378.023037	24.773914
143.626938	5366.989153	24.778931
143.310740	5380.751764	24.783949
143.304931	5388.942808	24.788967
143.938566	5406.557992	24.793984
143.633305	5421.629213	24.799002
143.804931	5432.846815	24.804019
143.964385	5439.200139	24.809037
144.357400	5457.413864	24.814055
144.386702	5462.373581	24.819072
145.033254	5472.398044	24.824090
145.062941	5474.859382	24.829107
145.016897	5494.043438	24.834125
145.353585	5492.719760	24.839143
145.449300	5492.838818	24.844160
145.483751	5511.390625	24.849178
145.740069	5516.258511	24.854195
145.989134	5538.821036	24.859213
145.782717	5536.306232	24.864231
146.133211	5539.767060	24.869248
146.734905	5554.231014	24.874266
147.146742	5555.270397	24.879283
147.108487	5557.064940	24.884301
147.078260	5555.477042	24.889319
147.339443	5551.859259	24.894336
147.243081	5547.823725	24.899354
147.212816	5551.880605	24.904371
147.711084	5569.797509	24.909389
147.628818	5574.097267	24.914407
147.959315	5570.187678	24.919424
147.958422	5580.188860	24.924442
148.120084	5581.288481	24.929459
148.068183	5602.161638	24.934477
148.143667	5612.981426	24.939495
148.165490	5607.083601	24.944512
148.259086	5624.306709	24.949530
148.896147	5633.568183	24.954547
148.754152	5635.611007	24.959565
148.973237	5646.612234	24.964583
149.322990	5661.264392	24.969600
149.069232	5672.680029	24.974618
149.385420	5671.297512	24.979635
149.817731	5675.329966	24.984653
149.528543	5693.010936	24.989671
149.911544	5694.487433	24.994688
149.830086	5700.436124	24.999706
150.040475	5706.733890	25.004723
150.065029	5722.721108	25.009741
150.162096	5735.962928	25.014759
150.709310	5750.136814	25.019776
150.894321	5764.076033	25.024794
151.165177	5759.221794	25.029811
151.041379	5757.958826	25.034829
151.170921	5775.159622	25.039847
151.417041	5797.887202	25.044864
151.479814	5793.324456	25.049882
152.027803	5775.518347	25.054899
152.047332	5808.378836	25.059917
152.004379	5813.619144	25.064935
152.350976	5820.770161	25.069952
152.414778	5813.531281	25.074970
152.472084	5809.749462	25.079987
152.524514	5823.572826	25.085005
152.826893	5835.139243	25.090023
153.448851	5842.884230	25.095040
153.252457	5846.243732	25.100058
153.234219	5845.007021	25.105075
153.346027	5843.900025	25.110093
153.259274	5852.281876	25.115111
153.566603	5867.525570	25.120128
153.422352	5866.755411	25.125146
154.029260	5883.896745	25.130163
154.234724	5900.857937	25.135181
153.872521	5908.301332	25.140199
154.463928	5900.396807	25.145216
154.355477	5919.460967	25.150234
154.535200	5919.067258	25.155251
154.956660	5922.638118	25.160269
154.806698	5938.022409	25.165287
155.305762	5942.952697	25.170304
155.147863	5956.953079	25.175322
155.962919	5951.849784	25.180339
156.326333	5946.464371	25.185357
156.093418	5953.265468	25.190375
156.604929	5953.391823	25.195392
156.597042	5974.470439	25.200410
156.852457	5974.505625	25.205427
156.741320	5982.949063	25.210445
156.859382	5979.074868	25.215463
157.213981	5977.150861	25.220480
156.938838	5980.079636	25.225498
156.896315	5970.136592	25.230515
156.822949	5989.683301	25.235533
156.878954	6010.705732	25.240551
157.825713	6015.211624	25.245568
157.460113	6024.438973	25.250586
157.804768	6043.648922	25.255603
158.061316	6052.347441	25.260621
157.779843	6058.000526	25.265639
158.337030	6074.344256	25.270656
158.443142	6069.099362	25.275674
158.601216	6094.489177	25.280691
158.407904	6098.119524	25.285709
158.301251	6116.690637	25.290727
158.847223	6131.669138	25.295744
158.871014	6145.143919	25.300762
159.145251	6160.251611	25.305779
159.407048	6152.379766	25.310797
160.214405	6166.315741	25.315815
160.257439	6174.742470	25.320832
160.393817	6180.800649	25.325850
160.465909	6180.802337	25.330867
160.568181	6178.982999	25.335885
160.342106	6197.444785	25.340903
160.967949	6197.589660	25.345920
161.198011	6208.587500	25.350938
161.010471	6219.433052	25.355955
161.237234	6205.413214	25.360973
161.414232	6237.419315	25.365991
161.808368	6249.685561	25.371008
161.740158	6240.502620	25.376026
161.714333	6233.357109	25.381043
161.751670	6248.659962	25.386061
161.993334	6262.197285	25.391079
162.516358	6259.756358	25.396096
162.746685	6277.380495	25.401114
162.834251	6286.829232	25.406131
163.009200	6304.060120	25.411149
162.860056	6307.018539	25.416167
163.148427	6291.462991	25.421184
163.334797	6306.716074	25.426202
163.296438	6328.461728	25.431219
163.653212	6330.925465	25.436237
163.655189	6333.225741	25.441255
163.914579	6346.095528	25.446272
164.148698	6366.598371	25.451290
164.398187	6364.453848	25.456307
164.502389	6366.738813	25.461325
164.586812	6371.851155	25.466343
164.752777	6386.889540	25.471360
164.907320	6394.967197	25.476378
164.381372	6399.647236	25.481395
165.260403	6414.712735	25.486413
165.003974	6426.307736	25.491431
165.385200	6427.493209	25.496448
165.232863	6446.623537	25.501466
165.346465	6454.145686	25.506483
165.676848	6475.048586	25.511501
166.140341	6485.705634	25.516519
166.465903	6480.386543	25.521536
166.725802	6507.977921	25.526554
166.920657	6503.356919	25.531571
167.329481	6509.675775	25.536589
167.166085	6515.541051	25.541607
167.279477	6518.754610	25.546624
167.510271	6540.311963	25.551642
167.359360	6548.655957	25.556659
167.964094	6548.891744	25.561677
167.945532	6562.353405	25.566695
168.140790	6573.091060	25.571712
168.603791	6584.345218	25.576730
168.404746	6582.113331	25.581747
168.619709	6594.768574	25.586765
168.931015	6610.418710	25.591783
169.013311	6606.621151	25.596800
169.027319	6608.735980	25.601818
169.259816	6625.480457	25.606835
169.527157	6627.274638	25.611853
169.669938	6640.405712	25.616871
169.949992	6647.687025	25.621888
170.112982	6657.503122	25.626906
170.273535	6665.104245	25.631923
170.444645	6669.803072	25.636941
170.419175	6670.260335	25.641959
170.560835	6680.941553	25.646976
170.551838	6700.827395	25.651994
170.168006	6710.812632	25.657011
171.111285	6714.158454	25.662029
171.337256	6728.023245	25.667047
171.628361	6748.421876	25.672064
171.568116	6748.560414	25.677082
171.655214	6758.086692	25.682100
172.197469	6766.947891	25.687117
172.298143	6787.359923	25.692135
172.411981	6778.724656	25.697152
172.374582	6791.988010	25.702170
172.558305	6818.295411	25.707188
173.189444	6806.013312	25.712205
173.378871	6810.906045	25.717223
173.024160	6820.347061	25.722240
173.563048	6835.595178	25.727258
173.343699	6844.320002	25.732276
174.061252	6844.176451	25.737293
173.848887	6863.234509	25.742311
173.665307	6869.656119	25.747328
174.207090	6873.655049	25.752346
174.085699	6894.904076	25.757364
174.962421	6903.006007	25.762381
174.677561	6905.125366	25.767399
175.064466	6905.084490	25.772416
175.070880	6900.025120	25.777434
174.852934	6923.225182	25.782452
175.429907	6927.241938	25.787469
175.739977	6937.758469	25.792487
175.592677	6946.369061	25.797504
175.839127	6959.552579	25.802522
175.761704	6964.319336	25.807540
175.915618	6974.802626	25.812557
176.434363	6986.893711	25.817575
176.400474	7000.744186	25.822592
176.829260	7018.048113	25.827610
176.603455	7029.841690	25.832628
177.207435	7031.110117	25.837645
177.430853	7049.014273	25.842663
177.257609	7057.333086	25.847680
177.366569	7055.455838	25.852698
177.775535	7086.666908	25.857716
177.982499	7094.694523	25.862733
177.963806	7093.824404	25.867751
178.206114	7113.608601	25.872768
178.567649	7112.259818	25.877786
178.563964	7129.527427	25.882804
179.098899	7141.849866	25.887821
179.389200	7149.915720	25.892839
179.149303	7144.893031	25.897856
179.625021	7161.195441	25.902874
179.126756	7173.042017	25.907892
179.696380	7181.988714	25.912909
180.286912	7202.371539	25.917927
180.290995	7210.104314	25.922944
180.895627	7204.975932	25.927962
180.911654	7223.832084	25.932980
181.097761	7235.844433	25.937997
181.089314	7234.458324	25.943015
181.303516	7244.939708	25.948032
181.385842	7243.661463	25.953050
181.187021	7267.093569	25.958068
181.756315	7263.617842	25.963085
181.764000	7278.987238	25.968103
181.649083	7303.033237	25.973120
182.322426	7303.184460	25.978138
182.082961	7329.596503	25.983156
182.449891	7344.198567	25.988173
182.542387	7345.553896	25.993191
182.992095	7377.489690	25.998208
183.250051	7370.701595	26.003226
183.235965	7376.262925	26.008244
183.641649	7393.466334	26.013261
183.976050	7410.414547	26.018279
183.938337	7401.156581	26.023296
184.266999	7415.781574	26.028314
184.254039	7428.738991	26.033332
184.456693	7437.401503	26.038349
184.811454	7437.076106	26.043367
184.657870	7460.625463	26.048384
185.253400	7462.126877	26.053402
185.271618	7464.251364	26.058420
185.671982	7473.714501	26.063437
185.651273	7485.798230	26.068455
185.723247	7487.752382	26.073472
185.736999	7496.483943	26.078490
185.634868	7514.407763	26.083508
185.922575	7523.228753	26.088525
186.275957	7547.830975	26.093543
186.394518	7548.661414	26.098560
186.752455	7561.574197	26.103578
187.024237	7582.868662	26.108596
187.360844	7583.710331	26.113613
187.432480	7580.588484	26.118631
187.404004	7590.547063	26.123648
187.858031	7595.358517	26.128666
187.809754	7605.617301	26.133684
187.797030	7612.947437	26.138701
188.131224	7626.389525	26.143719
188.185916	7633.770752	26.148736
188.391954	7646.575598	26.153754
188.370016	7668.025034	26.158772
188.674908	7672.212169	26.163789
189.311655	7700.708185	26.168807
189.325045	7709.669903	26.173824
189.624335	7710.051484	26.178842
189.603534	7725.945840	26.183860
189.893675	7740.509765	26.188877
190.507804	7744.996310	26.193895
190.293198	7758.318896	26.198912
190.672237	7765.779700	26.203930
190.663763	7779.444721	26.208948
190.790364	7786.301406	26.213965
191.009567	7797.847177	26.218983
191.535202	7808.512975	26.224000
191.658797	7822.479919	26.229018
191.902723	7829.624405	26.234036
192.161555	7826.479456	26.239053
192.486044	7834.039093	26.244071
192.261041	7840.115090	26.249088
192.486806	7862.481597	26.254106
192.768473	7864.662636	26.259124
192.918393	7872.118816	26.264141
193.093884	7891.614161	26.269159
193.315920	7883.700771	26.274176
193.702930	7886.600826	26.279194
194.209096	7922.147476	26.284212
194.317833	7916.791271	26.289229
194.321196	7921.144860	26.294247
194.253240	7935.187660	26.299264
194.463464	7935.913186	26.304282
194.836589	7951.071634	26.309300
194.702331	7958.739420	26.314317
195.157568	7961.270638	26.319335
195.034550	7985.442668	26.324352
195.225283	7975.778016	26.329370
195.599133	8005.969655	26.334388
195.845114	8016.076909	26.339405
196.015945	8017.724949	26.344423
195.825443	8034.277749	26.349440
196.274847	8056.828902	26.354458
196.467125	8059.677676	26.359476
196.562014	8083.290084	26.364493
196.983480	8083.179703	26.369511
196.552945	8105.068999	26.374528
197.296176	8107.531392	26.379546
197.350648	8125.152785	26.384564
197.315855	8129.350485	26.389581
197.738011	8152.629317	26.394599
198.271683	8161.052443	26.399616
198.183205	8173.131353	26.404634
198.391451	8188.358227	26.409652
198.214286	8196.197831	26.414669
199.195948	8211.096095	26.419687
199.256334	8229.339641	26.424704
199.514753	8221.567358	26.429722
199.520933	8244.648048	26.434740
199.965766	8261.045704	26.439757
200.300731	8253.555332	26.444775
200.192167	8261.252886	26.449792
200.623541	8252.052391	26.454810
201.043265	8264.978384	26.459828
201.169329	8283.679783	26.464845
201.520728	8280.196521	26.469863
201.489536	8288.199509	26.474880
201.580664	8287.013454	26.479898
201.793799	8284.939270	26.484916
201.884931	8283.267246	26.489933
202.068977	8297.960271	26.494951
202.040704	8315.272618	26.499968
202.290374	8316.132632	26.504986
202.226038	8336.345516	26.510004
202.378633	8335.929849	26.515021
202.615328	8348.782971	26.520039
202.722682	8380.824619	26.525056
202.753841	8385.381679	26.530074
203.174502	8404.881257	26.535092
203.215554	8423.674055	26.540109
203.608453	8428.225707	26.545127
203.966131	8450.051408	26.550144
204.235631	8469.738295	26.555162
204.516438	8477.882013	26.560180
204.580391	8502.062533	26.565197
204.767337	8513.803980	26.570215
205.075197	8522.800995	26.575232
205.030033	8534.724159	26.580250
205.240943	8555.191937	26.585268
205.355535	8574.672194	26.590285
205.816751	8580.802862	26.595303
205.680314	8602.140155	26.600320
205.918652	8612.672020	26.605338
206.537934	8633.396938	26.610356
206.177523	8648.015627	26.615373
207.063800	8662.179449	26.620391
207.090967	8668.635490	26.625408
207.066376	8689.792165	26.630426
207.630494	8697.325227	26.635444
208.057747	8715.797787	26.640461
208.319522	8727.555384	26.645479
208.034809	8738.469124	26.650496
208.305416	8752.974986	26.655514
208.677136	8755.937592	26.660532
208.615398	8782.590491	26.665549
209.397130	8792.597909	26.670567
209.126545	8796.474783	26.675584
209.500919	8821.450445	26.680602
209.847828	8817.770108	26.685620
210.028410	8836.447397	26.690637
210.478428	8846.150483	26.695655
210.604048	8860.904882	26.700672
210.642189	8859.039124	26.705690
211.133765	8872.214458	26.710708
211.269505	8881.857644	26.715725
211.517679	8889.316973	26.720743
211.778598	8891.839493	26.725760
211.335223	8906.457947	26.730778
211.956080	8907.577246	26.735796
212.165033	8925.434721	26.740813
212.342747	8942.232455	26.745831
212.283709	8947.385088	26.750848
212.570325	8964.955669	26.755866
213.020726	8972.172894	26.760884
212.872154	8982.342804	26.765901
213.479976	8996.992453	26.770919
213.370471	9012.492379	26.775936
213.482758	9025.890405	26.780954
214.136049	9036.334302	26.785972
213.940995	9044.422243	26.790989
214.127863	9054.380818	26.796007
214.249150	9071.074586	26.801024
214.251918	9086.710418	26.806042
214.852014	9099.021264	26.811060
214.713835	9116.918980	26.816077
215.069864	9126.747253	26.821095
215.720770	9148.159988	26.826112
215.808446	9153.014336	26.831130
215.964116	9171.117194	26.836148
215.895010	9186.891027	26.841165
216.157332	9190.493269	26.846183
216.597441	9216.351918	26.851200
216.699916	9229.289370	26.856218
217.114096	9231.192713	26.861236
217.234198	9261.183700	26.866253
217.391547	9261.251648	26.871271
217.942241	9268.255518	26.876288
218.337262	9286.734070	26.881306
218.725562	9292.717953	26.886324
218.774633	9294.416965	26.891341
218.676682	9305.182082	26.896359
219.009147	9324.054615	26.901376
218.762010	9336.142504	26.906394
218.911921	9345.726917	26.911412
219.087139	9368.873470	26.916429
219.536143	9387.016329	26.921447
219.867382	9399.285186	26.926464
219.963829	9416.567885	26.931482
220.351992	9421.645997	26.936500
220.373015	9446.359646	26.941517
220.752254	9455.059468	26.946535
221.013419	9474.959293	26.951552
221.053383	9496.048872	26.956570
221.278151	9506.092841	26.961588
221.190460	9515.205400	26.966605
221.895449	9534.569594	26.971623
221.964428	9551.307167	26.976640
222.276821	9588.144369	26.981658
222.799194	9581.863037	26.986676
223.134816	9598.361256	26.991693
222.907009	9614.691854	26.996711
223.309291	9623.944076	27.001728
223.612045	9647.439394	27.006746
223.673190	9643.306681	27.011764
224.218975	9659.217275	27.016781
224.202527	9688.796817	27.021799
224.624843	9688.142779	27.026816
224.944636	9697.485080	27.031834
225.190233	9707.921950	27.036852
225.153526	9708.142482	27.041869
225.149019	9724.900256	27.046887
225.870712	9732.557445	27.051904
225.971848	9748.651084	27.056922
226.570257	9761.185646	27.061940
226.391700	9766.618234	27.066957
226.627546	9777.457703	27.071975
226.706249	9780.583134	27.076992
226.768927	9810.704375	27.082010
227.237398	9819.030459	27.087028
227.581639	9838.933556	27.092045
227.690812	9838.858227	27.097063
227.740174	9851.941234	27.102080
227.837145	9867.158960	27.107098
228.053236	9884.135672	27.112116
228.217775	9903.512415	27.117133
228.105433	9925.852620	27.122151
228.617686	9941.001015	27.127168
228.434060	9960.339250	27.132186
229.142854	9974.464258	27.137204
229.511277	9986.165783	27.142221
229.353013	10000.937421	27.147239
229.945423	10024.337387	27.152256
230.038067	10046.272877	27.157274
230.257613	10047.476686	27.162292
230.870871	10069.162346	27.167309
230.642539	10081.643128	27.172327
231.035505	10092.100802	27.177344
231.270616	10115.404753	27.182362
231.660840	10124.269337	27.187380
231.643284	10132.048859	27.192397
231.898084	10145.807116	27.197415
232.153126	10156.004827	27.202432
232.620907	10176.900162	27.207450
233.211302	10183.405552	27.212468
233.471155	10195.422142	27.217485
233.258272	10200.940107	27.222503
233.846136	10217.832907	27.227520
233.765781	10233.230735	27.232538
234.135260	10237.438606	27.237556
234.589173	10251.402739	27.242573
234.626030	10250.531934	27.247591
234.781302	10271.341961	27.252608
234.946348	10286.926162	27.257626
235.095007	10298.429482	27.262644
235.689327	10317.530122	27.267661
235.997653	10313.450926	27.272679
236.238628	10320.214188	27.277696
236.398484	10349.894226	27.282714
236.570645	10354.861809	27.287732
236.960022	10361.514706	27.292749
237.341223	10374.007655	27.297767
237.091846	10381.303330	27.302784
237.090929	10394.220211	27.307802
237.433955	10415.997468	27.312820
237.903038	10425.358071	27.317837
237.857281	10444.878136	27.322855
238.225566	10462.408520	27.327872
238.333381	10469.033146	27.332890
238.782597	10494.444144	27.337908
239.158851	10506.932500	27.342925
239.069215	10518.339858	27.347943
239.904418	10525.816405	27.352960
239.721304	10553.465966	27.357978
239.923684	10566.640863	27.362996
240.053778	10576.890209	27.368013
240.200384	10598.857717	27.373031
240.588700	10618.473280	27.378048
240.802984	10626.552682	27.383066
241.011142	10650.303007	27.388084
241.354191	10665.668321	27.393101
241.446180	10674.710890	27.398119
241.794543	10698.319171	27.403136
241.751522	10716.567684	27.408154
242.184713	10728.096777	27.413172
242.516744	10744.824438	27.418189
242.501720	10770.170779	27.423207
242.990448	10781.417384	27.428224
243.093789	10811.118643	27.433242
243.595998	10807.692640	27.438260
244.042337	10834.289441	27.443277
244.032770	10840.984819	27.448295
244.576556	10847.406805	27.453312
244.807381	10876.436434	27.458330
244.825681	10868.863245	27.463348
245.244121	10883.266274	27.468365
245.185358	10901.563288	27.473383
245.567659	10906.668844	27.478400
245.507885	10926.178419	27.483418
245.799421	10934.306660	27.488436
245.842172	10950.067690	27.493453
245.976080	10973.553469	27.498471
246.503231	10978.354671	27.503488
246.586363	11007.849301	27.508506
247.128896	11023.691687	27.513524
247.525818	11029.652746	27.518541
247.505463	11061.958000	27.523559
247.726491	11063.507475	27.528576
247.927158	11087.280167	27.533594
248.316542	11103.228288	27.538612
248.619924	11118.496606	27.543629
248.920822	11138.966228	27.548647
249.305344	11142.157204	27.553664
249.371184	11154.086040	27.558682
249.540020	11165.868674	27.563700
249.697865	11184.400430	27.568717
249.575161	11205.007872	27.573735
249.955780	11211.879212	27.578752
250.616810	11237.492730	27.583770
250.482641	11260.934201	27.588788
251.029391	11270.406151	27.593805
251.297739	11296.431264	27.598823
251.741659	11307.236608	27.603840
252.174163	11330.869735	27.608858
252.146817	11340.698909	27.613876
252.534928	11349.006776	27.618893
252.545535	11382.323011	27.623911
252.557418	11382.237755	27.628928
253.084210	11415.888668	27.633946
253.066856	11437.097414	27.638964
253.680151	11445.916428	27.643981
253.804289	11476.868068	27.648999
254.496232	11472.440810	27.654016
254.625379	11496.442568	27.659034
254.853884	11509.520178	27.664052
255.305976	11521.218461	27.669069
255.324329	11542.959510	27.674087
255.612513	11537.663043	27.679104
255.821270	11564.051367	27.684122
255.919673	11589.266819	27.689140
256.482074	11596.618784	27.694157
256.581751	11623.579835	27.699175
256.798661	11627.552524	27.704192
257.404297	11657.264535	27.709210
257.615454	11661.168856	27.714228
258.237709	11660.591219	27.719245
258.408613	11681.555692	27.724263
258.634376	11681.224755	27.729280
259.022115	11703.537597	27.734298
258.760286	11722.623021	27.739316
259.355423	11705.469788	27.744333
259.371878	11725.295465	27.749351
259.316819	11743.406116	27.754368
259.635097	11755.465434	27.759386
259.590102	11788.520693	27.764404
260.195752	11798.416521	27.769421
260.322367	11816.516146	27.774439
260.193104	11836.029641	27.779456
260.828100	11848.911957	27.784474
260.972844	11875.170350	27.789492
261.332605	11889.560346	27.794509
261.604830	11915.967911	27.799527
261.952503	11923.914063	27.804544
261.837610	11932.834747	27.809562
262.317712	11963.627674	27.814580
262.541302	11972.507426	27.819597
263.090955	11994.096706	27.824615
262.590875	12009.917734	27.829632
263.090904	12022.342709	27.834650
263.280784	12039.645892	27.839668
263.657260	12059.871010	27.844685
263.930247	12081.615623	27.849703
264.233266	12099.075862	27.854720
264.977011	12114.316493	27.859738
265.141836	12129.165122	27.864756
266.018866	12135.773649	27.869773
265.836932	12147.217105	27.874791
266.284699	12169.507284	27.879808
266.708789	12181.824392	27.884826
266.843389	12176.330925	27.889844
267.105967	12187.815206	27.894861
267.265181	12190.560682	27.899879
267.531557	12202.041193	27.904896
268.172680	12216.707220	27.909914
268.169572	12235.340836	27.914932
268.266764	12233.328636	27.919949
268.263301	12256.335565	27.924967
268.307350	12262.790268	27.929984
268.684262	12287.485740	27.935002
268.827143	12304.755219	27.940020
269.253170	12323.412578	27.945037
269.431500	12348.479720	27.950055
269.561559	12365.368495	27.955072
270.012809	12382.397243	27.960090
270.296611	12405.825686	27.965108
270.833489	12427.478322	27.970125
270.777400	12448.422997	27.975143
271.345606	12470.859929	27.980160
271.500670	12477.821866	27.985178
271.549140	12502.823252	27.990196
272.041806	12512.387601	27.995213
272.355116	12539.041510	28.000231
272.349416	12564.319807	28.005248
272.761627	12572.770081	28.010266
273.012393	12604.721651	28.015284
273.386180	12619.788320	28.020301
273.296072	12634.920615	28.025319
273.669555	12665.307851	28.030336
274.115912	12681.459273	28.035354
273.976775	12703.934608	28.040372
274.803467	12721.698204	28.045389
274.893508	12736.118551	28.050407
275.091758	12760.091868	28.055424
275.905192	12776.863445	28.060442
276.195304	12793.143214	28.065460
276.761639	12818.283282	28.070477
277.034772	12829.936454	28.075495
276.843140	12834.646617	28.080512
277.343387	12849.364860	28.085530
277.374232	12869.439316	28.090548
277.760268	12885.454368	28.095565
278.059436	12897.125347	28.100583
277.994466	12914.428243	28.105600
278.214481	12926.840304	28.110618
278.276585	12958.028003	28.115636
278.729246	12975.352594	28.120653
279.180189	13005.667797	28.125671
279.488259	13016.795341	28.130688
279.896524	13034.607929	28.135706
280.069320	13066.800201	28.140724
280.138285	13073.216445	28.145741
280.288413	13096.137740	28.150759
280.724996	13107.474173	28.155776
281.106355	13135.380780	28.160794
281.415725	13153.332745	28.165812
281.431024	13170.761319	28.170829
281.894963	13184.272543	28.175847
282.277566	13201.511255	28.180864
282.150265	13219.144651	28.185882
282.768656	13252.202822	28.190900
282.695918	13260.022911	28.195917
283.235467	13272.577841	28.200935
283.303677	13290.045074	28.205952
283.422244	13310.942313	28.210970
283.883562	13345.369171	28.215988
284.156107	13367.356684	28.221005
284.470371	13384.772337	28.226023
284.692992	13407.310216	28.231040
285.028132	13437.355419	28.236058
285.318972	13461.024536	28.241076
285.641100	13482.666798	28.246093
285.850555	13508.218300	28.251111
285.552942	13531.768857	28.256128
286.353787	13555.869135	28.261146
286.413694	13589.434694	28.266164
286.872850	13608.456014	28.271181
287.232121	13633.582713	28.276199
287.769662	13663.423136	28.281216
288.517249	13684.349302	28.286234
288.347687	13708.329638	28.291252
288.754360	13730.185178	28.296269
289.286135	13748.318520	28.301287
289.550936	13760.802613	28.306304
290.004569	13789.804623	28.311322
290.167972	13802.853881	28.316340
290.255610	13825.082145	28.321357
290.926175	13828.028644	28.326375
291.235658	13851.750405	28.331392
291.666153	13861.810393	28.336410
291.912441	13882.696723	28.341428
292.061042	13893.249256	28.346445
292.442015	13905.964824	28.351463
292.272052	13922.077488	28.356480
292.571300	13940.857729	28.361498
292.922029	13968.080623	28.366516
293.731966	13983.412161	28.371533
293.606137	13998.165552	28.376551
293.895637	14024.687959	28.381568
294.270860	14045.641444	28.386586
294.608646	14066.755573	28.391604
295.062128	14071.720379	28.396621
295.211006	14094.320247	28.401639
295.368864	14105.233832	28.406656
295.682597	14121.889239	28.411674
295.816422	14156.753280	28.416692
295.988473	14173.165829	28.421709
296.375163	14195.767522	28.426727
296.813466	14225.335420	28.431744
297.115750	14230.421382	28.436762
297.005376	14261.220907	28.441780
297.327778	14283.281794	28.446797
297.944272	14299.488673	28.451815
298.113975	14334.003631	28.456832
298.637372	14349.537291	28.461850
298.659372	14370.078368	28.466868
298.697049	14388.119138	28.471885
299.270815	14409.311340	28.476903
299.327038	14433.288535	28.481920
299.790347	14454.702333	28.486938
299.995242	14474.089731	28.491956
300.331312	14505.490434	28.496973
301.091807	14500.235533	28.501991
301.068507	14547.229092	28.507008
301.147878	14550.355343	28.512026
301.636201	14572.226896	28.517044
302.092879	14603.218620	28.522061
302.182465	14608.604589	28.527079
302.643070	14637.643209	28.532096
303.102849	14650.997184	28.537114
302.910032	14675.676177	28.542132
303.470014	14701.475795	28.547149
304.263165	14711.640292	28.552167
304.027103	14737.921329	28.557184
304.461071	14758.908580	28.562202
304.772848	14784.946323	28.567220
304.857170	14794.796179	28.572237
305.315745	14816.055221	28.577255
305.704922	14839.557241	28.582272
305.782188	14862.335478	28.587290
306.052017	14890.413243	28.592308
306.299063	14919.454554	28.597325
306.867743	14923.943578	28.602343
307.005926	14961.169344	28.607360
307.311761	14974.325238	28.612378
307.632253	15014.652362	28.617396
307.860851	15039.848528	28.622413
308.091151	15061.028985	28.627431
308.217814	15096.214559	28.632448
308.604217	15125.368744	28.637466
309.053546	15150.267009	28.642484
309.353354	15186.303546	28.647501
309.772862	15205.092172	28.652519
310.328913	15234.648758	28.657536
310.681777	15257.738179	28.662554
310.866641	15269.462849	28.667572
311.027256	15308.981861	28.672589
311.198358	15329.575160	28.677607
311.845114	15353.701997	28.682624
312.293073	15379.412457	28.687642
312.577165	15403.953874	28.692660
312.705808	15424.321065	28.697677
312.902804	15458.258668	28.702695
312.873596	15477.769462	28.707712
313.573761	15495.772928	28.712730
314.425238	15528.863424	28.717748
314.554708	15548.617579	28.722765
314.981250	15562.203160	28.727783
314.960364	15588.921233	28.732800
315.507300	15607.385108	28.737818
315.851879	15615.238246	28.742836
316.179795	15662.082432	28.747853
316.593185	15673.867350	28.752871
316.732037	15692.833712	28.757888
317.215561	15701.593772	28.762906
317.762603	15719.109010	28.767924
318.122843	15742.713249	28.772941
318.593305	15749.694619	28.777959
318.684549	15770.002228	28.782976
318.809762	15789.981170	28.787994
319.370556	15809.520968	28.793012
319.512563	15817.957695	28.798029
319.649731	15841.238025	28.803047
319.909086	15861.410807	28.808064
319.783087	15888.219229	28.813082
320.730415	15906.374591	28.818100
320.988381	15931.050350	28.823117
320.718537	15961.658784	28.828135
321.209256	15975.355460	28.833152
321.333887	16004.529246	28.838170
321.840537	16023.016008	28.843188
321.876189	16047.331512	28.848205
322.331980	16062.975694	28.853223
322.718485	16095.382936	28.858240
322.867252	16117.393039	28.863258
323.255413	16141.540125	28.868276
323.752811	16154.079040	28.873293
324.782329	16184.539423	28.878311
324.528616	16209.396271	28.883328
324.693247	16229.268371	28.888346
325.100087	16246.695439	28.893364
325.294543	16279.391667	28.898381
326.007832	16294.692508	28.903399
326.415920	16322.379524	28.908416
326.472472	16349.070282	28.913434
327.273111	16359.563977	28.918452
327.221881	16383.992049	28.923469
327.202258	16401.444030	28.928487
327.164138	16433.335797	28.933504
327.323025	16470.386635	28.938522
328.363762	16498.587250	28.943540
328.217958	16530.142379	28.948557
328.657881	16558.188607	28.953575
329.180823	16583.031190	28.958592
329.598210	16621.094058	28.963610
329.875129	16639.130885	28.968628
330.251438	16672.949970	28.973645
330.589906	16694.584347	28.978663
330.944415	16721.322628	28.983680
331.554228	16762.068058	28.988698
331.807108	16778.815038	28.993716
331.763314	16818.664615	28.998733
332.317699	16848.943098	29.003751
332.508262	16865.656331	29.008768
333.250961	16898.934642	29.013786
333.704218	16921.343136	29.018804
333.784219	16932.487401	29.023821
334.380722	16971.041606	29.028839
334.710751	16986.136896	29.033856
334.794563	17000.938739	29.038874
335.551625	17023.018210	29.043892
335.282083	17053.294487	29.048909
336.361615	17079.051438	29.053927
336.466769	17094.122509	29.058944
336.660315	17121.028308	29.063962
337.207281	17144.353117	29.068980
337.113214	17161.599120	29.073997
337.739216	17187.442199	29.079015
337.989117	17206.639420	29.084032
338.173413	17223.908853	29.089050
338.558216	17254.958461	29.094068
338.806051	17279.366827	29.099085
339.138282	17302.965333	29.104103
339.175668	17335.051272	29.109120
339.143323	17369.219855	29.114138
340.240772	17397.595486	29.119156
340.478782	17414.678141	29.124173
340.866544	17451.321406	29.129191
341.114633	17483.022918	29.134208
341.320430	17503.201838	29.139226
341.912320	17529.929015	29.144244
342.336246	17572.199792	29.149261
343.055347	17581.204082	29.154279
342.889534	17605.500006	29.159296
343.268965	17643.746468	29.164314
343.679988	17650.111157	29.169332
343.988359	17694.374712	29.174349
344.333864	17704.591401	29.179367
344.518679	17726.999632	29.184384
344.487342	17754.525229	29.189402
345.274340	17779.587650	29.194420
345.860359	17799.247025	29.199437
345.957469	17828.433322	29.204455
346.372365	17841.408007	29.209472
346.902389	17865.836824	29.214490
346.882860	17880.427981	29.219508
347.165633	17915.693110	29.224525
347.550628	17936.894286	29.229543
347.954617	17953.934318	29.234560
348.373923	18000.033985	29.239578
348.704009	18018.602608	29.244596
348.632098	18056.295680	29.249613
349.138259	18080.768163	29.254631
349.613860	18101.997140	29.259648
349.581870	18135.946580	29.264666
349.980599	18159.683493	29.269684
350.495211	18194.535777	29.274701
351.181484	18226.160024	29.279719
351.967947	18246.486668	29.284736
352.275518	18277.281426	29.289754
352.770096	18284.475847	29.294772
352.969181	18310.533080	29.299789
353.297622	18333.846813	29.304807
353.612762	18348.540720	29.309824
354.002770	18388.703874	29.314842
354.149533	18401.330811	29.319860
354.766749	18438.028209	29.324877
354.678025	18458.515459	29.329895
355.110785	18484.896902	29.334912
355.260139	18519.654163	29.339930
356.204896	18546.171800	29.344948
356.237773	18572.469698	29.349965
356.583158	18610.880076	29.354983
357.207864	18626.492496	29.360000
357.130753	18655.757899	29.365018
357.526606	18673.331223	29.370036
357.999002	18705.048466	29.375053
358.155012	18740.274822	29.380071
358.801215	18762.007673	29.385088
358.743067	18807.777058	29.390106
359.161787	18833.388996	29.395124
359.523009	18862.839288	29.400141
359.526748	18899.399459	29.405159
360.177231	18926.325717	29.410176
360.506222	18971.047987	29.415194
360.861901	19000.430081	29.420212
361.125913	19026.595938	29.425229
361.727902	19065.146254	29.430247
362.442407	19092.431062	29.435264
362.699868	19124.211413	29.440282
363.104623	19147.181083	29.445300
363.853018	19170.923162	29.450317
363.748563	19201.652142	29.455335
364.524073	19214.527352	29.460352
364.884144	19257.410416	29.465370
365.122370	19268.306281	29.470388
365.410648	19288.729122	29.475405
365.637703	19324.863984	29.480423
366.186957	19343.911776	29.485440
366.452821	19377.196627	29.490458
366.826748	19390.940673	29.495476
367.492161	19412.713769	29.500493
367.705066	19447.434101	29.505511
368.346796	19464.012381	29.510528
368.739472	19481.806201	29.515546
368.925525	19516.450721	29.520564
369.053863	19518.168451	29.525581
369.367613	19551.481997	29.530599
370.036567	19567.426916	29.535616
369.803766	19585.757674	29.540634
369.924639	19619.729035	29.545652
370.454549	19640.771313	29.550669
370.390518	19683.780712	29.555687
370.671204	19716.359155	29.560704
370.785482	19755.049969	29.565722
371.430427	19800.825744	29.570740
371.606225	19832.628823	29.575757
372.229564	19880.774541	29.580775
372.865228	19911.847601	29.585792
372.757650	19953.693630	29.590810
373.363731	19988.668573	29.595828
373.873943	20024.226932	29.600845
373.891797	20067.859084	29.605863
374.350157	20092.780682	29.610880
374.730303	20141.251081	29.615898
375.338524	20184.024603	29.620916
375.805004	20212.637010	29.625933
376.202383	20244.434223	29.630951
376.613457	20277.064739	29.635968
376.829354	20329.492852	29.640986
377.378553	20363.708681	29.646004
378.338552	20390.348145	29.651021
378.336826	20422.564750	29.656039
379.150817	20449.819594	29.661056
379.433242	20485.703481	29.666074
380.085648	20509.679309	29.671092
380.798241	20523.518110	29.676109
381.232608	20547.572576	29.681127
381.927125	20569.302971	29.686144
381.811440	20598.647524	29.691162
381.977042	20618.899937	29.696180
382.583139	20635.677604	29.701197
382.583867	20662.416066	29.706215
383.243591	20685.394614	29.711232
383.355933	20718.720119	29.716250
383.519629	20746.978310	29.721268
383.982783	20771.712533	29.726285
384.341549	20808.487822	29.731303
384.673186	20839.686933	29.736320
384.881942	20864.903157	29.741338
385.049309	20906.146500	29.746356
385.647903	20938.786747	29.751373
385.868340	20975.243155	29.756391
386.598005	21006.580194	29.761408
386.920776	21046.264281	29.766426
387.085799	21082.909799	29.771444
387.802613	21113.741528	29.776461
388.324884	21142.931200	29.781479
388.430030	21170.219190	29.786496
389.050809	21201.079557	29.791514
389.286474	21227.261438	29.796532
389.645188	21254.701589	29.801549
389.900882	21294.184515	29.806567
390.455878	21330.397247	29.811584
390.612902	21361.902070	29.816602
391.046636	21400.545499	29.821620
391.393391	21439.397299	29.826637
391.807177	21460.784252	29.831655
392.617908	21506.352867	29.836672
392.911479	21534.499494	29.841690
393.621714	21553.595748	29.846708
393.769175	21590.000911	29.851725
394.346234	21613.749562	29.856743
394.493878	21631.333910	29.861760
394.932684	21664.068185	29.866778
395.292269	21685.251544	29.871796
395.763394	21710.430429	29.876813
395.839255	21744.525481	29.881831
396.112335	21764.876615	29.886848
396.298893	21806.163146	29.891866
396.794377	21845.281408	29.896884
397.501441	21877.681696	29.901901
397.458067	21913.047012	29.906919
397.860955	21941.535724	29.911936
398.472383	21969.512330	29.916954
398.613723	22009.603896	29.921972
399.281630	22039.628739	29.926989
398.899408	22094.190255	29.932007
399.559040	22120.765438	29.937024
400.372875	22164.888013	29.942042
400.930846	22206.881981	29.947060
401.297811	22225.058210	29.952077
401.635985	22284.461355	29.957095
402.082444	22302.112136	29.962112
402.610534	22336.625588	29.967130
402.946271	22390.451428	29.972148
403.325968	22409.970616	29.977165
403.834291	22437.824715	29.982183
404.391840	22474.239729	29.987200
404.561469	22509.694089	29.992218
404.982440	22559.099689	29.997236
405.663740	22589.657785	30.002253
405.719151	22630.603800	30.007271
406.334518	22665.128735	30.012288
406.665616	22694.497742	30.017306
407.104605	22739.156742	30.022324
407.272253	22765.304957	30.027341
407.863726	22809.019761	30.032359
408.247007	22853.506951	30.037376
408.954473	22892.089674	30.042394
409.266525	22930.017264	30.047412
409.549240	22950.355628	30.052429
409.892471	22986.294733	30.057447
410.369080	23021.619048	30.062464
410.788233	23057.014420	30.067482
410.925572	23095.512046	30.072500
411.530493	23129.265503	30.077517
411.966280	23169.844112	30.082535
412.219659	23213.852321	30.087552
412.722280	23259.821889	30.092570
412.772753	23301.858274	30.097588
413.566359	23333.720453	30.102605
414.181893	23383.868919	30.107623
414.342589	23418.003796	30.112640
415.061227	23454.890987	30.117658
415.342256	23487.874039	30.122676
416.156490	23530.555847	30.127693
416.301373	23555.072397	30.132711
416.926373	23579.702035	30.137728
417.722194	23616.393928	30.142746
417.903544	23645.303691	30.147764
418.189197	23673.686984	30.152781
418.675437	23711.406228	30.157799
419.125077	23737.741149	30.162816
419.399688	23770.864567	30.167834
419.621331	23805.250322	30.172852
420.466480	23834.544280	30.177869
420.725028	23865.623903	30.182887
421.101416	23902.533919	30.187904
421.505830	23937.277635	30.192922
421.677720	23963.258289	30.197940
422.076194	23987.976399	30.202957
422.493243	24022.929491	30.207975
422.743691	24052.055590	30.212992
423.244202	24088.001015	30.218010
423.375482	24126.583980	30.223028
423.855218	24159.789380	30.228045
424.305163	24195.118976	30.233063
424.489838	24228.918823	30.238080
424.758599	24274.918743	30.243098
424.746158	24308.344494	30.248116
425.639965	24361.182492	30.253133
426.314432	24412.940502	30.258151
426.635208	24449.217555	30.263168
427.118904	24495.788066	30.268186
427.570548	24537.833780	30.273204
427.926818	24577.744558	30.278221
428.327276	24622.987287	30.283239
428.567168	24659.006934	30.288256
429.505321	24698.257367	30.293274
429.748635	24745.405974	30.298292
430.697123	24785.000231	30.303309
430.919959	24824.479497	30.308327
431.263943	24854.392562	30.313344
432.273595	24890.241392	30.318362
432.513926	24931.842046	30.323380
432.802196	24969.254612	30.328397
433.507131	24992.007672	30.333415
433.604932	25033.993222	30.338432
434.387423	25075.654473	30.343450
434.821020	25104.455670	30.348468
435.265126	25129.809696	30.353485
435.420364	25180.564614	30.358503
435.848875	25214.516944	30.363520
436.590371	25240.906910	30.368538
436.745650	25289.363039	30.373556
437.295013	25321.245656	30.378573
437.573573	25363.307810	30.383591
437.949816	25398.259435	30.388608
438.878057	25430.062325	30.393626
438.681815	25472.982173	30.398644
439.244967	25505.411622	30.403661
439.649305	25552.176327	30.408679
440.000249	25593.323517	30.413696
440.608943	25622.167628	30.418714
440.851706	25680.094048	30.423732
440.927127	25720.973249	30.428749
441.861979	25759.258442	30.433767
442.292535	25806.930984	30.438784
442.855465	25835.718362	30.443802
443.252438	25883.421895	30.448820
443.852459	25919.668570	30.453837
444.531455	25954.927716	30.458855
444.851055	25996.882150	30.463872
445.252385	26023.277482	30.468890
445.698170	26065.003080	30.473908
446.116621	26089.610560	30.478925
446.495448	26135.072190	30.483943
446.837917	26178.688576	30.488960
447.754902	26206.191207	30.493978
447.894420	26259.035115	30.498996
448.066036	26289.474343	30.504013
448.538793	26325.052180	30.509031
448.987961	26378.939740	30.514048
449.032134	26419.991356	30.519066
449.241815	26470.487213	30.524084
449.506002	26516.609057	30.529101
450.335226	26561.152144	30.534119
450.241159	26601.022190	30.539136
451.092838	26656.651395	30.544154
451.793683	26709.713065	30.549172
452.005784	26750.791353	30.554189
452.433393	26791.938224	30.559207
452.707058	26834.261860	30.564224
453.495649	26897.692834	30.569242
454.341517	26924.407232	30.574260
454.705848	26965.952926	30.579277
455.353145	27004.528124	30.584295
455.468776	27045.594665	30.589312
455.934579	27076.387267	30.594330
456.476879	27133.627259	30.599348
457.058156	27175.317410	30.604365
457.726216	27213.955885	30.609383
457.606329	27256.156320	30.614400
458.179027	27300.936108	30.619418
458.227054	27350.388840	30.624436
459.064700	27394.875928	30.629453
459.737161	27437.097325	30.634471
459.814177	27494.450071	30.639488
460.557736	27536.275155	30.644506
460.950658	27592.106186	30.649524
460.980824	27654.387776	30.654541
461.577543	27695.739136	30.659559
462.245016	27740.734672	30.664576
462.898357	27780.436678	30.669594
463.228401	27835.736354	30.674612
463.930816	27882.663204	30.679629
464.511960	27925.556971	30.684647
464.869637	27971.623114	30.689664
465.335073	28008.133007	30.694682
465.447490	28052.482939	30.699700
466.047564	28107.171108	30.704717
466.808507	28135.497502	30.709735
467.609508	28195.108185	30.714752
467.757729	28234.957762	30.719770
468.334663	28275.134062	30.724788
468.847656	28333.016903	30.729805
469.528556	28365.713054	30.734823
469.520336	28420.098935	30.739840
470.333679	28461.031517	30.744858
470.712826	28509.458174	30.749876
470.937155	28558.443631	30.754893
471.398920	28582.788870	30.759911
471.554053	28649.280291	30.764928
472.187556	28701.822980	30.769946
472.822793	28748.861070	30.774964
473.192761	28794.889524	30.779981
473.793533	28843.286816	30.784999
473.988594	28899.195763	30.790016
474.804128	28942.759938	30.795034
475.109458	28992.676427	30.800052
475.482434	29046.793113	30.805069
476.164777	29088.543750	30.810087
476.971070	29128.371854	30.815104
477.097076	29173.741315	30.820122
477.857153	29222.655928	30.825140
478.176064	29271.839131	30.830157
478.924037	29307.585869	30.835175
479.148351	29363.172872	30.840192
479.750741	29409.312831	30.845210
479.977316	29450.278432	30.850228
480.407768	29499.551110	30.855245
481.143458	29532.489629	30.860263
481.668469	29587.743771	30.865280
482.365801	29624.581548	30.870298
483.161010	29662.854349	30.875316
483.227477	29715.099448	30.880333
484.029086	29724.645566	30.885351
484.383432	29770.710738	30.890368
484.708073	29792.676516	30.895386
485.223110	29833.787806	30.900404
485.663364	29869.510822	30.905421
486.332749	29910.003727	30.910439
486.594287	29949.680794	30.915456
486.959441	29985.296577	30.920474
486.950892	30035.706405	30.925492
487.143012	30082.821308	30.930509
487.730805	30124.088464	30.935527
488.096744	30187.475146	30.940544
488.496047	30231.827427	30.945562
489.327824	30295.686473	30.950580
489.843315	30345.411242	30.955597
490.149211	30387.798189	30.960615
490.561715	30459.348898	30.965632
491.009114	30512.104472	30.970650
491.753144	30554.397370	30.975668
491.776134	30633.171263	30.980685
492.436582	30675.247963	30.985703
493.131922	30740.449870	30.990720
493.512150	30783.967533	30.995738
494.389122	30837.782551	31.000756
494.571020	30903.599883	31.005773
495.364334	30950.595741	31.010791
496.091461	31002.372764	31.015808
496.660347	31048.661415	31.020826
497.322574	31089.672485	31.025844
497.618708	31157.431063	31.030861
498.329426	31191.370631	31.035879
499.103637	31243.181604	31.040896
499.323311	31283.127317	31.045914
499.763039	31331.226870	31.050932
500.316290	31383.147317	31.055949
500.858895	31424.163156	31.060967
501.159087	31485.943785	31.065984
501.619368	31527.068110	31.071002
502.205974	31577.737429	31.076020
501.977490	31638.690989	31.081037
502.599021	31678.681649	31.086055
503.290930	31744.512547	31.091072
503.620881	31802.329892	31.096090
504.118041	31856.863864	31.101108
504.501324	31928.750369	31.106125
505.338297	31984.067837	31.111143
505.653285	32045.523025	31.116160
506.015699	32114.959134	31.121178
506.613746	32164.956237	31.126196
507.035173	32231.537212	31.131213
507.936107	32278.439983	31.136231
508.586766	32336.890763	31.141248
508.692612	32401.331732	31.146266
509.273738	32450.745598	31.151284
509.753778	32521.006290	31.156301
510.672300	32572.163177	31.161319
511.041957	32630.642417	31.166336
511.245308	32691.509361	31.171354
512.063043	32742.749650	31.176372
512.407942	32815.867160	31.181389
513.032518	32863.946687	31.186407
513.375887	32916.666730	31.191424
513.815681	32970.008350	31.196442
514.557443	33031.099897	31.201460
514.905742	33096.355261	31.206477
515.703339	33148.537153	31.211495
516.365277	33206.749160	31.216512
516.412794	33259.736804	31.221530
517.166306	33298.885834	31.226548
517.311049	33365.204422	31.231565
518.033551	33418.383957	31.236583
518.454650	33477.349725	31.241600
518.938234	33528.205752	31.246618
519.803022	33573.817968	31.251636
520.258049	33634.987364	31.256653
520.652194	33671.599764	31.261671
521.170847	33741.814762	31.266688
521.466549	33798.142375	31.271706
522.291833	33843.146522	31.276724
522.712694	33909.692902	31.281741
523.050972	33965.679547	31.286759
523.928301	34012.644476	31.291776
524.297470	34072.232945	31.296794
524.604478	34130.481374	31.301812
524.922877	34198.194323	31.306829
525.798966	34251.534007	31.311847
526.073513	34312.246461	31.316864
526.174664	34383.665758	31.321882
527.208846	34435.578870	31.326900
527.461736	34517.269865	31.331917
527.735739	34584.732871	31.336935
528.470526	34653.934428	31.341952
528.709107	34724.186951	31.346970
529.133346	34796.043640	31.351988
529.550147	34877.731304	31.357005
529.628630	34949.257590	31.362023
530.625578	35024.816719	31.367040
531.006816	35102.629961	31.372058
531.821495	35184.420557	31.377076
532.470232	35256.178910	31.382093
533.909289	35337.819748	31.387111
534.487018	35409.006658	31.392128
534.900492	35461.994066	31.397146
535.656289	35523.577850	31.402164
536.048168	35583.047712	31.407181
536.857469	35649.984544	31.412199
537.433727	35704.053421	31.417216
538.243571	35753.855270	31.422234
538.771062	35817.812981	31.427252
539.588702	35868.775158	31.432269
539.867275	35931.111335	31.437287
540.221500	35974.516693	31.442304
540.612992	36029.150389	31.447322
541.663058	36086.424122	31.452340
541.741614	36150.652830	31.457357
542.501260	36200.053967	31.462375
542.950283	36247.060828	31.467392
543.407316	36313.619678	31.472410
543.954231	36369.137604	31.477428
544.473522	36442.187572	31.482445
545.025305	36494.495634	31.487463
545.519579	36549.606247	31.492480
545.909792	36614.839184	31.497498
546.779820	36659.776794	31.502516
547.309963	36730.803253	31.507533
547.581113	36790.805160	31.512551
548.338715	36850.067344	31.517568
548.711691	36915.503040	31.522586
549.383828	36970.639219	31.527604
549.931537	37027.225743	31.532621
550.253200	37089.277952	31.537639
550.637011	37148.066352	31.542656
551.062347	37217.717128	31.547674
551.493211	37273.550521	31.552692
552.035507	37352.754489	31.557709
552.904406	37402.655317	31.562727
553.613928	37471.591072	31.567744
553.983627	37528.249601	31.572762
554.564537	37566.884227	31.577780
555.110660	37640.625798	31.582797
555.403909	37692.134237	31.587815
556.108765	37741.589697	31.592832
556.257199	37819.828750	31.597850
556.840874	37878.453968	31.602868
557.412462	37958.757223	31.607885
558.341801	38019.553991	31.612903
558.925516	38076.049493	31.617920
559.321927	38149.069877	31.622938
559.984044	38198.972348	31.627956
560.723140	38267.480186	31.632973
560.930471	38330.909526	31.637991
561.560965	38392.085146	31.643008
562.395241	38466.195950	31.648026
562.914347	38527.620825	31.653044
563.132600	38594.353790	31.658061
563.623895	38675.352067	31.663079
564.507134	38740.274549	31.668096
564.739081	38811.869760	31.673114
565.423754	38876.765560	31.678132
566.019870	38951.163871	31.683149
566.510182	39013.182208	31.688167
567.385935	39076.345944	31.693184
567.621465	39155.965138	31.698202
568.481752	39231.848605	31.703220
569.024158	39298.495901	31.708237
569.460226	39372.452084	31.713255
570.148534	39440.035320	31.718272
570.790464	39521.072462	31.723290
571.140394	39589.823174	31.728308
571.852637	39645.320717	31.733325
572.005791	39735.643490	31.738343
572.835762	39800.998363	31.743360
573.625116	39883.404737	31.748378
573.808154	39948.939589	31.753396
574.915573	40020.969431	31.758413
574.959469	40104.617301	31.763431
575.817472	40168.497964	31.768448
576.338041	40243.463262	31.773466
577.067098	40313.536616	31.778484
577.697407	40384.696599	31.783501
577.991875	40465.637505	31.788519
578.662069	40531.592716	31.793536
579.534829	40613.802380	31.798554
580.024843	40696.186108	31.803572
580.335783	40762.741257	31.808589
580.860336	40845.138890	31.813607
581.626078	40912.162396	31.818624
581.929223	40988.293556	31.823642
582.941445	41059.307859	31.828660
583.492317	41126.812721	31.833677
583.944189	41212.263831	31.838695
584.687238	41277.679385	31.843712
585.251610	41355.312523	31.848730
586.252066	41428.659813	31.853748
586.839635	41495.484445	31.858765
587.636692	41569.850778	31.863783
587.869425	41618.706608	31.868800
588.367639	41690.628995	31.873818
589.379415	41758.700871	31.878836
590.043985	41818.846963	31.883853
589.914905	41892.628890	31.888871
590.777762	41954.882952	31.893888
591.591529	42023.812428	31.898906
592.236785	42074.176564	31.903924
592.872353	42144.348127	31.908941
593.289984	42199.283350	31.913959
593.784182	42252.987564	31.918976
594.009180	42321.260919	31.923994
594.770430	42388.306343	31.929012
595.358106	42448.776564	31.934029
595.897078	42518.851862	31.939047
596.311906	42588.452301	31.944064
596.809982	42661.587584	31.949082
597.484969	42728.089723	31.954100
598.347196	42807.049883	31.959117
598.341128	42887.182943	31.964135
598.971967	42948.389549	31.969152
599.588271	43030.500854	31.974170
600.000803	43109.359788	31.979188
600.873781	43187.101212	31.984205
601.179547	43269.728942	31.989223
601.692817	43355.246147	31.994240
602.026400	43440.073625	31.999258
602.988341	43529.678475	32.004276
603.718437	43600.291412	32.009293
604.529557	43691.585714	32.014311
605.343569	43763.615560	32.019328
606.025559	43835.572779	32.024346
606.699141	43922.676235	32.029364
607.272237	43985.935289	32.034381
607.939262	44070.975778	32.039399
608.446073	44148.544928	32.044416
608.923131	44218.046499	32.049434
609.846260	44300.084338	32.054452
610.491730	44373.934497	32.059469
611.024300	44452.031063	32.064487
611.761575	44521.269787	32.069504
612.105678	44599.000290	32.074522
612.616396	44675.794319	32.079540
613.368998	44760.085035	32.084557
614.126797	44833.946882	32.089575
614.479807	44913.558944	32.094592
615.079520	44990.487963	32.099610
615.667566	45075.811296	32.104628
616.694903	45154.356357	32.109645
616.906002	45244.387107	32.114663
617.874154	45316.877423	32.119680
618.346029	45402.603472	32.124698
618.677913	45480.459641	32.129716
619.425755	45557.600175	32.134733
620.044963	45646.327768	32.139751
620.867813	45722.222055	32.144768
621.340183	45800.968843	32.149786
621.873924	45890.639987	32.154804
622.771353	45965.304176	32.159821
623.005894	46053.775170	32.164839
623.323606	46142.873810	32.169856
624.324883	46225.917596	32.174874
624.961742	46317.872399	32.179892
625.634743	46396.538031	32.184909
625.921650	46480.765007	32.189927
626.722387	46561.393158	32.194944
627.107246	46648.515959	32.199962
627.584972	46744.155575	32.204980
628.835079	46833.052975	32.209997
629.373673	46923.899712	32.215015
629.850767	46999.853111	32.220032
630.738483	47084.021451	32.225050
631.518663	47177.421923	32.230068
631.882154	47246.344065	32.235085
632.453520	47330.622590	32.240103
633.256925	47407.900484	32.245120
633.786953	47488.533106	32.250138
634.457273	47567.797719	32.255156
635.101212	47645.889192	32.260173
635.196761	47723.705260	32.265191
636.198796	47799.313088	32.270208
636.956333	47882.549692	32.275226
637.328404	47964.271437	32.280244
637.939071	48038.353340	32.285261
638.869453	48133.524196	32.290279
639.202683	48208.293616	32.295296
639.995341	48290.859917	32.300314
640.775854	48389.113585	32.305332
641.606730	48453.336693	32.310349
642.214544	48544.896620	32.315367
642.818005	48624.160909	32.320384
643.559839	48696.654253	32.325402
644.056457	48779.284203	32.330420
644.601850	48861.514875	32.335437
645.086278	48953.172937	32.340455
645.631626	49030.992710	32.345472
646.425546	49133.315454	32.350490
647.014538	49219.317400	32.355508
647.877952	49300.104775	32.360525
648.465628	49385.706624	32.365543
649.039241	49483.652738	32.370560
649.896039	49549.021631	32.375578
650.667174	49659.318689	32.380596
651.364771	49735.322420	32.385613
651.739072	49823.330022	32.390631
652.334622	49914.159566	32.395648
652.956984	49996.875086	32.400666
653.683127	50094.338058	32.405684
654.554432	50178.440723	32.410701
655.089920	50280.540698	32.415719
655.844142	50360.936878	32.420736
656.055704	50448.923702	32.425754
656.912472	50556.994749	32.430772
658.183113	50637.079411	32.435789
658.455192	50719.214783	32.440807
658.981499	50819.073642	32.445824
659.682237	50897.421729	32.450842
659.617292	50993.924008	32.455860
661.086126	51095.798381	32.460877
661.649616	51189.298543	32.465895
662.088833	51295.096082	32.470912
662.670048	51381.124815	32.475930
663.355068	51482.994879	32.480948
664.237556	51570.095918	32.485965
664.700093	51667.796756	32.490983
665.535040	51770.249988	32.496000
666.478736	51864.243356	32.501018
667.016729	51947.401280	32.506036
667.653407	52040.871378	32.511053
668.254038	52128.103606	32.516071
669.037534	52216.613636	32.521088
670.175316	52317.497376	32.526106
670.417301	52429.091632	32.531124
671.188937	52504.680327	32.536141
671.643423	52597.958952	32.541159
672.309264	52684.266943	32.546176
673.368333	52768.798436	32.551194
674.068501	52866.529258	32.556212
674.735392	52940.052289	32.561229
675.951324	53022.689099	32.566247
676.431224	53111.758737	32.571264
677.279405	53193.616816	32.576282
677.673105	53270.275358	32.581300
678.236091	53350.222837	32.586317
678.867646	53427.821903	32.591335
679.530410	53506.509030	32.596352
680.492738	53582.493699	32.601370
680.783305	53659.107631	32.606388
681.413089	53750.619236	32.611405
681.702124	53828.276466	32.616423
682.132946	53921.262113	32.621440
682.991480	54002.698616	32.626458
683.338934	54107.967565	32.631476
683.975719	54195.133617	32.636493
684.671522	54303.719687	32.641511
685.329982	54392.329776	32.646528
686.029124	54500.670000	32.651546
686.650485	54598.732100	32.656564
687.443744	54690.694944	32.661581
687.964181	54799.287455	32.666599
688.689831	54910.089505	32.671616
689.669137	54998.238695	32.676634
690.187177	55108.393824	32.681652
691.231882	55202.541443	32.686669
691.837163	55310.263537	32.691687
691.971712	55424.047093	32.696704
692.901148	55508.182254	32.701722
693.659930	55621.358422	32.706740
694.573939	55725.518973	32.711757
695.060706	55822.377391	32.716775
695.744038	55936.003780	32.721792
696.626733	56035.729484	32.726810
696.614420	56145.068187	32.731828
697.630881	56251.002654	32.736845
698.448092	56364.748407	32.741863
699.087591	56470.487256	32.746880
699.960187	56574.975053	32.751898
700.367957	56688.556508	32.756916
701.629104	56802.307289	32.761933
702.098870	56914.868857	32.766951
703.053947	57021.759048	32.771968
703.689839	57123.862532	32.776986
704.502199	57228.351092	32.782004
705.162534	57321.782492	32.787021
705.734152	57439.909541	32.792039
706.610712	57550.303435	32.797056
707.536871	57643.382836	32.802074
708.337625	57744.021625	32.807092
708.970334	57854.508030	32.812109
709.643759	57961.456117	32.817127
710.507869	58061.112954	32.822144
711.518848	58157.712983	32.827162
711.879185	58266.161430	32.832180
712.963415	58363.925678	32.837197
713.869717	58466.484282	32.842215
714.248316	58557.844847	32.847232
715.324800	58647.826778	32.852250
716.122200	58754.411103	32.857268
716.746179	58839.407069	32.862285
717.353609	58934.744182	32.867303
717.834075	59041.906864	32.872320
718.792292	59132.656170	32.877338
718.974109	59232.387298	32.882356
719.748319	59334.567745	32.887373
721.052897	59422.967289	32.892391
721.555724	59526.387870	32.897408
722.508893	59619.212943	32.902426
722.772814	59723.678766	32.907444
723.428015	59820.206562	32.912461
724.591819	59922.489972	32.917479
725.226562	60018.946269	32.922496
725.881474	60104.233186	32.927514
726.457693	60186.196765	32.932532
726.512810	60293.676515	32.937549
727.712821	60379.746678	32.942567
727.888120	60485.368612	32.947584
728.899556	60581.291428	32.952602
729.326908	60679.592550	32.957620
729.936855	60780.966963	32.962637
730.736934	60890.981140	32.967655
730.868516	60999.564291	32.972672
731.437644	61108.644550	32.977690
732.515230	61239.596503	32.982708
733.010613	61363.971667	32.987725
734.122532	61466.713874	32.992743
734.903868	61584.173439	32.997760
735.674647	61694.241063	33.002778
736.627322	61808.779090	33.007796
737.355364	61927.216405	33.012813
737.931989	62036.350981	33.017831
738.772236	62141.328217	33.022848
739.609104	62257.518489	33.027866
740.757331	62361.801351	33.032884
741.346821	62474.216325	33.037901
741.882416	62590.584654	33.042919
742.758987	62701.442935	33.047936
743.239870	62814.516070	33.052954
744.347714	62923.946900	33.057972
744.877564	63042.467675	33.062989
745.878556	63149.901159	33.068007
746.508545	63270.524062	33.073024
747.098247	63387.140816	33.078042
748.036791	63499.965194	33.083060
748.625948	63627.031242	33.088077
749.448623	63736.930675	33.093095
749.798174	63855.947340	33.098112
750.990111	63975.356524	33.103130
751.809634	64098.866838	33.108148
752.157021	64217.645770	33.113165
752.973810	64341.461390	33.118183
753.720580	64455.523644	33.123200
754.305177	64576.073229	33.128218
755.222464	64697.459828	33.133236
755.710736	64826.964539	33.138253
757.074462	64953.759179	33.143271
757.559488	65082.260994	33.148288
758.040024	65198.501508	33.153306
759.047361	65316.324449	33.158324
759.967530	65443.163739	33.163341
760.811936	65575.838111	33.168359
761.424233	65695.005321	33.173376
762.355106	65814.784340	33.178394
763.125671	65928.439923	33.183412
763.431794	66046.167891	33.188429
764.517430	66172.807329	33.193447
765.358420	66306.852357	33.198464
766.179095	66429.700034	33.203482
767.147733	66547.909335	33.208500
767.433214	66672.730622	33.213517
768.436375	66791.207429	33.218535
768.913488	66913.172786	33.223552
769.684102	67043.472845	33.228570
770.532021	67155.206913	33.233588
771.221018	67292.678111	33.238605
772.111807	67414.628660	33.243623
773.168394	67539.865146	33.248640
774.145954	67663.857395	33.253658
775.148839	67769.999658	33.258676
775.464550	67897.282463	33.263693
776.335274	68009.769637	33.268711
777.188853	68119.396408	33.273728
778.055129	68233.510256	33.278746
778.902569	68330.014733	33.283764
779.167726	68449.450990	33.288781
780.028617	68555.235033	33.293799
780.799260	68683.496946	33.298816
781.194037	68806.074878	33.303834
782.374258	68920.855018	33.308852
782.392841	69053.144155	33.313869
783.041778	69163.575153	33.318887
783.527845	69297.691623	33.323904
784.330834	69442.523545	33.328922
785.376117	69575.082652	33.333940
786.112858	69712.606057	33.338957
787.341070	69842.399028	33.343975
788.171099	69974.661096	33.348992
788.595951	70118.055331	33.354010
789.745664	70246.934333	33.359028
790.385036	70391.300281	33.364045
791.277967	70513.869077	33.369063
792.001805	70653.038281	33.374080
793.020701	70780.140154	33.379098
793.880911	70920.736497	33.384116
794.158455	71057.035626	33.389133
794.864200	71187.896814	33.394151
796.025602	71335.843900	33.399168
796.703098	71479.388955	33.404186
797.621653	71610.154362	33.409204
798.130921	71764.655222	33.414221
799.371986	71902.052598	33.419239
799.717347	72041.002491	33.424256
800.267581	72190.346326	33.429274
801.361722	72336.806536	33.434292
801.888551	72474.818734	33.439309
803.190832	72625.862509	33.444327
804.068630	72763.945076	33.449344
804.911535	72907.459735	33.454362
805.731806	73050.972764	33.459380
806.203020	73192.571474	33.464397
807.450625	73334.909228	33.469415
808.173285	73483.841516	33.474432
808.938553	73632.179703	33.479450
809.799812	73770.448509	33.484468
810.766970	73910.009710	33.489485
811.780526	74051.891270	33.494503
812.425998	74190.135153	33.499520
813.341986	74334.317543	33.504538
814.430556	74467.804111	33.509556
815.175773	74602.891219	33.514573
816.076542	74740.584221	33.519591
817.210690	74880.946205	33.524608
817.916809	75019.349776	33.529626
818.867169	75137.312626	33.534644
819.096353	75274.595010	33.539661
820.151841	75416.592393	33.544679
820.721660	75552.258225	33.549696
821.417150	75694.209348	33.554714
822.372893	75836.833055	33.559732
822.783980	75990.191352	33.564749
823.639992	76131.005734	33.569767
824.439073	76284.105969	33.574784
825.231172	76434.805157	33.579802
826.058002	76576.013004	33.584820
826.834352	76723.655754	33.589837
827.813843	76876.603841	33.594855
828.561079	77022.684927	33.599872
829.357369	77167.310550	33.604890
830.229148	77308.983700	33.609908
830.665995	77461.184273	33.614925
831.216469	77596.568671	33.619943
831.920360	77732.042410	33.624960
833.046252	77892.474536	33.629978
833.627316	78036.192667	33.634996
834.487664	78194.583631	33.640013
835.443898	78346.856332	33.645031
836.536023	78485.306544	33.650048
837.245714	78644.497245	33.655066
837.955509	78794.720130	33.660084
838.814439	78948.404537	33.665101
839.634481	79097.131186	33.670119
840.674923	79258.302037	33.675136
841.130018	79409.121415	33.680154
842.346843	79565.755472	33.685172
843.224249	79723.471376	33.690189
843.927963	79865.637694	33.695207
844.741961	80028.856638	33.700224
845.516218	80192.734857	33.705242
846.680862	80357.460686	33.710260
847.582415	80515.507108	33.715277
848.045744	80671.602812	33.720295
848.996746	80821.438931	33.725312
850.201022	80977.224643	33.730330
851.042386	81143.527779	33.735348
851.929456	81298.627983	33.740365
852.409359	81447.192338	33.745383
853.969190	81615.297041	33.750400
854.575176	81779.031147	33.755418
855.366860	81936.068228	33.760436
856.255028	82093.874890	33.765453
857.210842	82251.734742	33.770471
858.142779	82416.678518	33.775488
858.633017	82580.001024	33.780506
859.748676	82727.070726	33.785524
860.673090	82908.087782	33.790541
861.682062	83063.856849	33.795559
862.466976	83215.178630	33.800576
863.453033	83383.397505	33.805594
864.463332	83534.620926	33.810612
865.181354	83693.592879	33.815629
866.020257	83853.178625	33.820647
866.795594	83999.964774	33.825664
867.713259	84174.761367	33.830682
868.462490	84326.880891	33.835700
869.819154	84496.476571	33.840717
870.344595	84661.851655	33.845735
871.342314	84810.238558	33.850752
872.005969	84981.002479	33.855770
872.705231	85144.726346	33.860788
873.490890	85305.273670	33.865805
873.991758	85472.784461	33.870823
875.032407	85636.746488	33.875840
875.663114	85821.378131	33.880858
876.468520	85999.819835	33.885876
877.522522	86184.068123	33.890893
878.251573	86347.681697	33.895911
879.629605	86517.193789	33.900928
880.331560	86701.270202	33.905946
881.047165	86868.040635	33.910964
882.273583	87028.444861	33.915981
882.915904	87219.988837	33.920999
883.702134	87386.093264	33.926016
884.933418	87570.190377	33.931034
885.558502	87740.000200	33.936052
886.916539	87907.678063	33.941069
887.293152	88083.194590	33.946087
888.429730	88238.433296	33.951104
889.051153	88405.635215	33.956122
890.160038	88576.472235	33.961140
890.951885	88728.917280	33.966157
891.672556	88896.112626	33.971175
892.587689	89066.814343	33.976192
893.303238	89231.279258	33.981210
894.217710	89405.324686	33.986228
895.172889	89585.540836	33.991245
895.891570	89751.135241	33.996263
896.901330	89919.720242	34.001280
897.770145	90098.423147	34.006298
899.016955	90264.712304	34.011316
899.919916	90437.007965	34.016333
900.834864	90609.113045	34.021351
901.872031	90778.566595	34.026368
902.530556	90949.311576	34.031386
903.252810	91125.268224	34.036404
904.200089	91302.631910	34.041421
905.067548	91478.567184	34.046439
905.955465	91667.701806	34.051456
906.798571	91846.789114	34.056474
907.594966	92024.164070	34.061492
908.781630	92211.057596	34.066509
909.538085	92397.878046	34.071527
910.536516	92574.312358	34.076544
911.550858	92766.586511	34.081562
912.376597	92943.007733	34.086580
912.855316	93127.303818	34.091597
913.620528	93326.876568	34.096615
915.156984	93519.190756	34.101632
915.870393	93719.718328	34.106650
916.812666	93904.234926	34.111668
918.044641	94093.971008	34.116685
918.951159	94286.888968	34.121703
920.316734	94457.731941	34.126720
921.362640	94651.693102	34.131738
922.135596	94826.611351	34.136756
923.296418	95002.555479	34.141773
923.878967	95188.077952	34.146791
925.152343	95359.290580	34.151808
925.970177	95557.917159	34.156826
926.641369	95745.100226	34.161844
928.003169	95917.359203	34.166861
928.983030	96101.753265	34.171879
929.775256	96267.671388	34.176896
930.572175	96454.478295	34.181914
931.772572	96629.997122	34.186932
932.759856	96818.984484	34.191949
933.352618	97005.139301	34.196967
934.410471	97170.798084	34.201984
935.220128	97366.338870	34.207002
935.675207	97563.243743	34.212020
936.971227	97741.691836	34.217037
937.551510	97931.463852	34.222055
938.427833	98119.390642	34.227072
939.547243	98317.932620	34.232090
940.320441	98517.666474	34.237108
941.297191	98716.931518	34.242125
942.074576	98909.292881	34.247143
943.518643	99106.724004	34.252160
944.137202	99293.974170	34.257178
945.163796	99488.508193	34.262196
946.669280	99666.327705	34.267213
947.385422	99855.028317	34.272231
948.781806	100039.756278	34.277248
949.496093	100224.465262	34.282266
950.389401	100401.612347	34.287284
951.777788	100580.211006	34.292301
952.463899	100755.413212	34.297319
953.660750	100927.917616	34.302336
954.441946	101093.432746	34.307354
955.096537	101261.622567	34.312372
956.250141	101440.323026	34.317389
957.020294	101620.746806	34.322407
957.733510	101788.373287	34.327424
958.905085	101966.029822	34.332442
959.614475	102148.854239	34.337460
960.751174	102328.032222	34.342477
961.408777	102526.120019	34.347495
962.368678	102709.742821	34.352512
963.130641	102896.932566	34.357530
963.984691	103086.280174	34.362548
965.113004	103277.977220	34.367565
966.051612	103482.427186	34.372583
967.284285	103656.343364	34.377600
968.344397	103861.320793	34.382618
969.058836	104053.497158	34.387636
970.478763	104236.485030	34.392653
971.410809	104443.470060	34.397671
972.695198	104632.162756	34.402688
973.889301	104809.885845	34.407706
974.477747	104998.930384	34.412724
975.407337	105185.368171	34.417741
976.181860	105395.198191	34.422759
977.254284	105585.313178	34.427776
978.287865	105775.803225	34.432794
979.057869	105967.794581	34.437812
980.041357	106157.181204	34.442829
981.296130	106365.749251	34.447847
982.875387	106552.862059	34.452864
983.645040	106739.805908	34.457882
984.447417	106934.623226	34.462900
985.826703	107128.143565	34.467917
986.682364	107318.230888	34.472935
987.437094	107505.993189	34.477952
988.677464	107699.895272	34.482970
989.273313	107908.634959	34.487988
990.335204	108092.791745	34.493005
991.036874	108290.852682	34.498023
992.177840	108503.420685	34.503040
993.308483	108696.499558	34.508058
994.143394	108906.702153	34.513076
995.363044	109100.149224	34.518093
995.828420	109306.983515	34.523111
997.033800	109517.421061	34.528128
998.294182	109719.402827	34.533146
998.988316	109923.328874	34.538164
1000.115948	110119.445739	34.543181
1001.381522	110329.411047	34.548199
1001.982519	110532.445091	34.553216
1003.040208	110739.483931	34.558234
1003.961618	110953.931579	34.563252
1005.145501	111148.336612	34.568269
1006.058443	111352.604657	34.573287
1007.402168	111556.423106	34.578304
1008.608178	111767.739436	34.583322
1009.499505	111963.465311	34.588340
1010.971210	112167.140530	34.593357
1011.806983	112367.134696	34.598375
1012.396031	112558.734489	34.603392
1013.384311	112762.481284	34.608410
1014.158741	112976.234380	34.613428
1015.718972	113170.642354	34.618445
1016.258167	113381.308489	34.623463
1017.369200	113588.740166	34.628480
1018.125105	113778.674073	34.633498
1019.133762	113975.281684	34.638516
1020.494478	114165.498445	34.643533
1021.276186	114363.311759	34.648551
1021.945652	114561.297036	34.653568
1023.186870	114772.985357	34.658586
1023.932529	114980.741147	34.663604
1024.945493	115177.305887	34.668621
1025.805120	115390.164073	34.673639
1026.959820	115597.679565	34.678656
1027.882009	115809.504434	34.683674
1028.467016	116030.052231	34.688692
1029.089422	116245.464562	34.693709
1030.467213	116479.618420	34.698727
1031.553996	116682.870925	34.703744
1033.019881	116911.680018	34.708762
1033.839879	117149.263602	34.713780
1035.117615	117358.912938	34.718797
1036.044874	117576.705013	34.723815
1036.928908	117797.876087	34.728832
1038.249366	118018.685423	34.733850
1039.323032	118249.850669	34.738868
1040.301980	118465.297049	34.743885
1041.079195	118690.319082	34.748903
1042.313051	118914.139836	34.753920
1043.558735	119146.943762	34.758938
1044.646036	119381.270855	34.763956
1045.918101	119597.652997	34.768973
1047.241269	119826.040235	34.773991
1048.161509	120046.804573	34.779008
1049.465771	120262.692229	34.784026
1050.370326	120491.914101	34.789044
1051.470439	120706.267554	34.794061
1052.639703	120921.092683	34.799079
1053.533350	121157.962393	34.804096
1054.627314	121371.396757	34.809114
1055.437263	121597.196326	34.814132
1057.092886	121827.952040	34.819149
1058.034753	122047.676258	34.824167
1059.117421	122256.443074	34.829184
1059.922730	122476.953364	34.834202
1060.986181	122716.785570	34.839220
1062.227193	122943.031222	34.844237
1063.257827	123158.440561	34.849255
1064.107725	123381.750823	34.854272
1065.205466	123614.792298	34.859290
1066.229069	123853.170306	34.864308
1067.312287	124071.314872	34.869325
1068.475933	124302.399280	34.874343
1069.446939	124532.921661	34.879360
1070.844353	124752.628796	34.884378
1071.512189	124976.183853	34.889396
1072.643566	125207.724150	34.894413
1073.773347	125454.943255	34.899431
1074.730682	125675.490201	34.904448
1075.947874	125904.854569	34.909466
1076.884459	126154.696690	34.914484
1077.896421	126383.148061	34.919501
1079.233446	126616.122701	34.924519
1079.783207	126839.533642	34.929536
1081.617077	127078.183713	34.934554
1082.368973	127325.797348	34.939572
1083.626076	127544.407320	34.944589
1084.908727	127781.569639	34.949607
1085.622526	128019.334675	34.954624
1086.613151	128242.315558	34.959642
1087.772196	128481.176716	34.964660
1088.778233	128711.180117	34.969677
1089.778850	128933.910876	34.974695
1090.881578	129159.224710	34.979712
1092.092707	129388.996512	34.984730
1093.074415	129618.414969	34.989748
1093.962229	129837.875376	34.994765
1095.295827	130066.719382	34.999783
1096.273300	130295.281629	35.004800
1097.109753	130525.389868	35.009818
1097.870125	130772.180518	35.014836
1099.203312	131002.425750	35.019853
1100.249400	131242.049306	35.024871
1101.251334	131470.058370	35.029888
1102.382543	131708.644700	35.034906
1103.364370	131966.740331	35.039924
1104.859816	132216.273047	35.044941
1106.325497	132453.516842	35.049959
1107.241649	132697.863054	35.054976
1108.460811	132920.497374	35.059994
1108.909415	133175.318979	35.065012
1110.262115	133422.729756	35.070029
1111.689443	133677.938897	35.075047
1112.446046	133926.795692	35.080064
1113.465976	134167.421758	35.085082
1114.858432	134417.216884	35.090100
1115.947129	134668.027541	35.095117
1117.545236	134902.263208	35.100135
1118.720455	135159.731531	35.105152
1119.819351	135398.185948	35.110170
1121.065670	135637.416454	35.115188
1122.190073	135894.429933	35.120205
1123.364757	136132.851872	35.125223
1124.199902	136390.576241	35.130240
1125.458721	136638.229973	35.135258
1126.698320	136888.360924	35.140276
1127.567796	137151.359580	35.145293
1128.887551	137392.099468	35.150311
1129.667936	137652.860146	35.155328
1130.739329	137894.811084	35.160346
1132.243350	138155.481625	35.165364
1133.239346	138415.490049	35.170381
1134.612515	138661.073497	35.175399
1135.685269	138923.989276	35.180416
1136.892326	139175.296623	35.185434
1137.824015	139427.500792	35.190452
1138.956543	139689.842173	35.195469
1140.236383	139931.469178	35.200487
1140.961406	140207.625883	35.205504
1142.328513	140460.019494	35.210522
1143.709193	140718.131103	35.215540
1145.026518	140974.429305	35.220557
1146.199256	141226.214058	35.225575
1147.257220	141489.431226	35.230592
1148.519641	141733.952215	35.235610
1149.744560	141995.472007	35.240628
1150.483987	142255.108559	35.245645
1151.881899	142508.437883	35.250663
1153.155024	142781.621252	35.255680
1154.047233	143028.596415	35.260698
1154.991938	143291.541762	35.265716
1156.271382	143545.557621	35.270733
1157.554046	143805.876974	35.275751
1158.583398	144072.580343	35.280768
1160.040951	144327.396741	35.285786
1161.578870	144598.065289	35.290804
1162.400461	144852.356451	35.295821
1163.607942	145095.261724	35.300839
1164.617923	145369.776906	35.305856
1166.092689	145604.551104	35.310874
1166.943633	145860.518594	35.315892
1168.226197	146094.148418	35.320909
1169.569879	146345.726453	35.325927
1170.280458	146589.079077	35.330944
1171.321925	146818.454455	35.335962
1172.371060	147080.003221	35.340980
1173.481199	147334.125044	35.345997
1175.097049	147582.775437	35.351015
1176.115728	147845.526894	35.356032
1177.268347	148090.199058	35.361050
1178.289434	148346.676201	35.366068
1179.248804	148611.040948	35.371085
1180.062615	148862.026539	35.376103
1180.981584	149136.129033	35.381120
1182.640158	149398.824162	35.386138
1184.173902	149664.864598	35.391156
1185.218241	149941.945505	35.396173
1186.621636	150209.584046	35.401191
1187.616316	150478.141742	35.406208
1188.578146	150742.014152	35.411226
1190.078688	151014.994664	35.416244
1191.067413	151296.229554	35.421261
1192.833975	151554.800224	35.426279
1193.789965	151832.759633	35.431296
1194.777127	152108.610528	35.436314
1196.012620	152372.449312	35.441332
1196.699958	152660.276166	35.446349
1197.763310	152935.372222	35.451367
1199.119992	153225.211063	35.456384
1200.345313	153520.629309	35.461402
1201.955210	153804.431339	35.466420
1202.803300	154092.876732	35.471437
1203.881781	154382.326368	35.476455
1204.811383	154683.637113	35.481472
1206.208377	154973.165475	35.486490
1207.523728	155270.434279	35.491508
1208.620577	155561.196244	35.496525
1210.186869	155858.301300	35.501543
1211.037941	156151.873498	35.506560
1212.588066	156451.218254	35.511578
1214.284276	156742.942957	35.516596
1215.095824	157040.917320	35.521613
1216.337951	157325.275234	35.526631
1217.557066	157629.973287	35.531648
1218.980235	157914.952511	35.536666
1220.499619	158214.962708	35.541684
1221.535052	158521.879814	35.546701
1222.704167	158799.790788	35.551719
1223.949459	159097.861246	35.556736
1225.034747	159400.438385	35.561754
1226.440963	159690.126794	35.566772
1227.461697	159997.488936	35.571789
1228.908579	160288.278596	35.576807
1230.319098	160594.489935	35.581824
1231.447284	160880.566469	35.586842
1232.917941	161174.453965	35.591860
1234.031530	161472.956910	35.596877
1235.675263	161755.541835	35.601895
1236.746889	162054.855177	35.606912
1237.761449	162343.726325	35.611930
1238.856180	162635.263151	35.616948
1240.002024	162948.056675	35.621965
1241.359744	163239.808064	35.626983
1242.419616	163529.035192	35.632000
1243.535351	163829.470469	35.637018
1244.878298	164123.767861	35.642036
1245.641347	164425.001452	35.647053
1247.246590	164739.229583	35.652071
1248.391957	165024.646644	35.657088
1249.945391	165313.220895	35.662106
1251.092128	165603.589738	35.667124
1252.010676	165884.431691	35.672141
1253.171494	166179.572677	35.677159
1253.944272	166476.391088	35.682176
1255.111737	166778.005877	35.687194
1256.714274	167078.053763	35.692212
1257.880643	167387.273097	35.697229
1259.144875	167680.567443	35.702247
1260.558455	167990.892179	35.707264
1261.835513	168303.652435	35.712282
1263.274576	168600.286485	35.717300
1264.343631	168911.029837	35.722317
1266.189741	169206.826760	35.727335
1267.313978	169514.456500	35.732352
1268.036078	169820.873158	35.737370
1269.610240	170122.583266	35.742388
1270.476445	170447.924963	35.747405
1271.550229	170753.401690	35.752423
1273.229947	171074.210505	35.757440
1274.470659	171401.870111	35.762458
1275.852317	171711.286888	35.767476
1277.256783	172042.756243	35.772493
1278.639368	172356.758108	35.777511
1279.769931	172673.493906	35.782528
1280.747306	173004.901076	35.787546
1282.365191	173313.172909	35.792564
1283.822183	173645.749079	35.797581
1285.153833	173968.132869	35.802599
1286.500623	174291.353915	35.807616
1287.406943	174620.766523	35.812634
1288.713475	174936.486057	35.817652
1289.672131	175276.503613	35.822669
1291.072487	175609.877054	35.827687
1292.605559	175939.753715	35.832704
1293.773206	176279.388557	35.837722
1295.463024	176611.832826	35.842740
1296.397213	176948.198626	35.847757
1297.995673	177270.662162	35.852775
1299.417106	177601.698039	35.857792
1300.282667	177937.092076	35.862810
1301.975486	178273.430602	35.867828
1303.030010	178608.721865	35.872845
1304.406955	178948.391432	35.877863
1305.814104	179275.201977	35.882880
1307.317597	179618.789534	35.887898
1308.619263	179952.145300	35.892916
1310.276373	180289.556684	35.897933
1311.218811	180614.675786	35.902951
1312.937955	180948.921078	35.907968
1314.142650	181289.903997	35.912986
1316.162352	181608.784912	35.918004
1316.873608	181937.618530	35.923021
1318.538646	182268.073714	35.928039
1320.336307	182583.113494	35.933056
1321.459975	182907.277916	35.938074
1323.108619	183225.265377	35.943092
1324.373930	183552.862718	35.948109
1325.535037	183875.656141	35.953127
1327.119418	184192.340006	35.958144
1327.832142	184506.262995	35.963162
1329.396495	184831.178784	35.968180
1330.528221	185160.280402	35.973197
1331.783379	185485.758879	35.978215
1332.876821	185820.709551	35.983232
1333.889964	186169.625174	35.988250
1335.015236	186486.169782	35.993268
1335.944997	186820.722020	35.998285
1336.967988	187136.500266	36.003303
1338.482824	187465.958702	36.008320
1339.655383	187807.013880	36.013338
1341.062634	188139.895881	36.018356
1342.132262	188485.034081	36.023373
1343.056195	188808.593869	36.028391
1344.795017	189150.858472	36.033408
1345.768275	189515.237114	36.038426
1347.290598	189861.768735	36.043444
1348.690530	190209.198522	36.048461
1349.970963	190557.805271	36.053479
1351.157488	190915.899401	36.058496
1352.443212	191283.830030	36.063514
1353.995918	191638.364546	36.068532
1355.658299	192009.639603	36.073549
1356.766771	192367.082630	36.078567
1358.155760	192737.518734	36.083584
1359.646828	193104.512744	36.088602
1361.293101	193451.920935	36.093620
1362.631990	193831.740662	36.098637
1363.716931	194187.649593	36.103655
1365.356060	194559.147282	36.108672
1366.309158	194934.327705	36.113690
1367.956957	195290.404002	36.118708
1369.031679	195680.726699	36.123725
1370.323794	196051.427297	36.128743
1371.957487	196416.081546	36.133760
1372.971299	196805.481798	36.138778
1374.698640	197184.458006	36.143796
1376.235898	197570.107549	36.148813
1377.479403	197937.107336	36.153831
1378.915960	198328.948043	36.158848
1380.290991	198707.331120	36.163866
1381.931146	199081.762322	36.168884
1383.469422	199462.979333	36.173901
1385.011547	199847.562305	36.178919
1386.649832	200223.142858	36.183936
1387.735328	200608.122932	36.188954
1389.320312	200986.001801	36.193972
1391.044425	201351.963468	36.198989
1392.140290	201730.079509	36.204007
1393.547746	202114.024593	36.209024
1394.467330	202486.295441	36.214042
1396.081080	202880.139268	36.219060
1397.406516	203264.091484	36.224077
1398.557773	203652.810351	36.229095
1400.223060	204041.611554	36.234112
1401.235926	204436.616960	36.239130
1402.746496	204837.344822	36.244148
1404.082791	205218.423477	36.249165
1404.895777	205615.118828	36.254183
1406.883188	206011.838338	36.259200
1408.115297	206406.729251	36.264218
1410.104822	206799.008601	36.269236
1411.813384	207174.893461	36.274253
1414.345110	207557.107241	36.279271
1415.953486	207930.612561	36.284288
1417.569739	208300.055217	36.289306
1419.130544	208672.137149	36.294324
1420.858712	209030.149774	36.299341
1422.455745	209390.763269	36.304359
1423.885764	209742.276365	36.309376
1425.197005	210091.474231	36.314394
1426.639617	210441.794724	36.319412
1428.169767	210788.584993	36.324429
1429.215196	211149.602122	36.329447
1430.824668	211480.433730	36.334464
1431.829708	211827.162650	36.339482
1432.969235	212177.413557	36.344500
1434.542555	212512.737612	36.349517
1435.506419	212859.134729	36.354535
1436.924092	213202.207635	36.359552
1437.997229	213558.367125	36.364570
1439.053234	213916.156282	36.369588
1440.209982	214272.279500	36.374605
1441.249740	214650.086873	36.379623
1442.782804	215020.398572	36.384640
1444.220545	215396.492640	36.389658
1445.186828	215788.488440	36.394676
1446.659079	216165.367313	36.399693
1447.666797	216579.429799	36.404711
1448.920102	216966.938742	36.409728
1450.287670	217377.897713	36.414746
1451.673204	217786.061773	36.419764
1453.325358	218196.621765	36.424781
1453.988874	218663.272658	36.429799
1456.156234	219099.200090	36.434816
1457.759411	219530.092151	36.439834
1458.982181	219954.318345	36.444852
1461.190522	220347.245423	36.449869
1462.676353	220761.297699	36.454887
1464.565119	221180.898219	36.459904
1465.871498	221590.995888	36.464922
1467.199916	222004.139369	36.469940
1468.795895	222420.846938	36.474957
1469.313454	222830.698606	36.479975
1471.036453	223264.354929	36.484992
1472.697556	223693.552953	36.490010
1474.349428	224118.055323	36.495028
1476.065222	224555.502379	36.500045
1477.590036	224980.714754	36.505063
1479.365780	225396.210112	36.510080
1480.865072	225838.980886	36.515098
1482.336537	226246.046039	36.520116
1483.966768	226677.901915	36.525133
1485.355557	227112.770962	36.530151
1486.711933	227533.041969	36.535168
1488.090196	227961.565791	36.540186
1489.427626	228403.585262	36.545204
1491.092247	228826.756164	36.550221
1492.916964	229261.636958	36.555239
1494.883366	229679.299803	36.560256
1495.809382	230118.243390	36.565274
1497.483491	230553.381900	36.570292
1498.980537	230959.695975	36.575309
1500.433882	231409.428168	36.580327
1502.029962	231836.353801	36.585344
1503.828531	232266.498611	36.590362
1504.922602	232705.117847	36.595380
1506.760351	233123.980747	36.600397
1508.254171	233573.611423	36.605415
1509.933454	233985.339794	36.610432
1511.633431	234412.458966	36.615450
1513.292797	234834.200949	36.620468
1515.037987	235245.159743	36.625485
1516.528545	235684.941355	36.630503
1518.025839	236101.048900	36.635520
1519.278629	236516.893013	36.640538
1520.775577	236944.712798	36.645556
1522.405338	237363.849777	36.650573
1523.776094	237793.800811	36.655591
1524.683717	238208.461244	36.660608
1526.719441	238642.826088	36.665626
1528.044371	239069.434658	36.670644
1529.638906	239497.168192	36.675661
1530.755056	239919.672598	36.680679
1531.993216	240333.343275	36.685696
1533.760267	240749.569349	36.690714
1535.232802	241171.509539	36.695732
1536.655136	241588.505438	36.700749
1538.175127	242012.751072	36.705767
1539.927009	242433.377543	36.710784
1541.449171	242853.509260	36.715802
1542.989713	243275.543892	36.720820
1544.669465	243699.664712	36.725837
1546.030707	244120.460308	36.730855
1547.716184	244545.419935	36.735872
1549.383108	244975.463846	36.740890
1550.519846	245424.190644	36.745908
1552.466130	245841.386966	36.750925
1554.213918	246273.172399	36.755943
1555.693710	246699.947572	36.760960
1557.526534	247139.417292	36.765978
1558.787298	247556.221155	36.770996
1560.444085	247996.330815	36.776013
1561.889633	248443.080671	36.781031
1563.257166	248872.925680	36.786048
1564.776517	249308.436423	36.791066
1566.487869	249769.242743	36.796084
1567.785720	250209.084199	36.801101
1569.388296	250660.713667	36.806119
1571.023126	251118.943099	36.811136
1572.668253	251570.439513	36.816154
1573.995662	252032.480276	36.821172
1575.877087	252484.700690	36.826189
1576.350666	252958.035174	36.831207
1578.021528	253425.583838	36.836224
1579.495680	253898.169770	36.841242
1581.002368	254381.851895	36.846260
1582.572274	254855.261054	36.851277
1584.270166	255342.595783	36.856295
1585.874625	255827.355108	36.861312
1586.975476	256325.940963	36.866330
1588.465190	256821.693964	36.871348
1590.230026	257316.334865	36.876365
1591.649348	257815.910406	36.881383
1593.561205	258325.820203	36.886400
1595.167097	258821.554785	36.891418
1596.902383	259331.493978	36.896436
1598.984056	259827.810738	36.901453
1600.289667	260324.916082	36.906471
1601.816322	260821.654731	36.911488
1602.956666	261320.590989	36.916506
1604.835374	261832.183242	36.921524
1606.523040	262340.834754	36.926541
1608.476344	262838.341093	36.931559
1609.959612	263349.693434	36.936576
1611.487715	263869.751530	36.941594
1613.021695	264364.379775	36.946612
1614.493560	264882.719283	36.951629
1615.984520	265397.270280	36.956647
1617.273162	265912.337012	36.961664
1619.116247	266429.115552	36.966682
1620.823586	266953.664084	36.971700
1622.952125	267461.579835	36.976717
1624.425042	267981.746031	36.981735
1626.387615	268500.560797	36.986752
1627.859433	269012.343152	36.991770
1629.398521	269538.466603	36.996788
1630.679928	270049.847403	37.001805
1632.623218	270564.725624	37.006823
1634.297826	271081.070099	37.011840
1635.939234	271594.472631	37.016858
1637.600270	272101.291869	37.021876
1639.650187	272585.158244	37.026893
1640.906444	273075.988242	37.031911
1642.542916	273562.410900	37.036928
1644.145074	274061.031793	37.041946
1645.589626	274572.404631	37.046964
1647.225788	275065.734477	37.051981
1648.803026	275570.555170	37.056999
1650.470091	276071.676741	37.062016
1652.427771	276581.132249	37.067034
1653.552938	277093.264347	37.072052
1655.110112	277598.770291	37.077069
1656.760537	278112.134523	37.082087
1658.279183	278645.434778	37.087104
1660.043160	279157.609443	37.092122
1661.702632	279692.357302	37.097140
1663.471307	280204.274709	37.102157
1665.427961	280737.116546	37.107175
1666.818266	281259.635611	37.112192
1669.002834	281777.602324	37.117210
1670.408362	282318.176819	37.122228
1672.565109	282824.511237	37.127245
1674.511320	283349.041222	37.132263
1676.306536	283881.875523	37.137280
1677.782287	284393.525215	37.142298
1679.047811	284914.530415	37.147316
1681.123952	285459.125173	37.152333
1682.846282	285980.127879	37.157351
1683.961382	286521.753281	37.162368
1685.948740	287050.913365	37.167386
1687.195865	287582.759273	37.172404
1688.852680	288142.502186	37.177421
1690.238964	288679.757056	37.182439
1691.916145	289243.302555	37.187456
1693.971083	289788.901438	37.192474
1695.323075	290350.413326	37.197492
1697.154559	290899.854797	37.202509
1699.484620	291457.339894	37.207527
1700.678256	292023.189016	37.212544
1702.579843	292565.372950	37.217562
1704.065845	293141.303597	37.222580
1705.898433	293698.429290	37.227597
1707.102981	294261.066243	37.232615
1708.861362	294837.833045	37.237632
1710.600132	295402.433911	37.242650
1712.461917	295985.680355	37.247668
1713.787952	296561.163859	37.252685
1716.062030	297129.757267	37.257703
1717.581234	297709.241520	37.262720
1719.666732	298273.364557	37.267738
1721.369166	298858.781238	37.272756
1723.659672	299428.477536	37.277773
1725.501555	299986.459860	37.282791
1726.964383	300565.556963	37.287808
1729.192331	301124.612363	37.292826
1730.588357	301688.373567	37.297844
1731.975935	302272.095745	37.302861
1733.972879	302833.440071	37.307879
1735.170559	303421.351934	37.312896
1737.099697	303990.573957	37.317914
1738.802191	304565.417343	37.322932
1740.305524	305154.461647	37.327949
1742.116626	305732.962440	37.332967
1743.676820	306318.561252	37.337984
1745.496556	306895.503944	37.343002
1747.234090	307486.653071	37.348020
1748.910302	308073.186177	37.353037
1750.697134	308648.091000	37.358055
1752.355552	309234.161958	37.363072
1754.039673	309790.232147	37.368090
1755.627543	310360.536051	37.373108
1757.326713	310916.570784	37.378125
1759.321879	311493.021480	37.383143
1760.440815	312064.609755	37.388160
1762.347480	312639.111358	37.393178
1763.798357	313227.117759	37.398196
1765.825309	313816.243613	37.403213
1767.853221	314396.019676	37.408231
1769.676367	314985.017773	37.413248
1771.338032	315565.505530	37.418266
1773.183258	316155.963608	37.423284
1774.854857	316738.446627	37.428301
1776.547248	317329.301355	37.433319
1778.342923	317926.685624	37.438336
1780.002493	318525.483950	37.443354
1781.687022	319135.090361	37.448372
1783.152025	319741.325075	37.453389
1785.098771	320354.127766	37.458407
1787.133542	320989.864814	37.463424
1788.532447	321599.928147	37.468442
1790.278001	322222.827638	37.473460
1791.678086	322847.936529	37.478477
1793.967760	323474.441572	37.483495
1795.587130	324105.799229	37.488512
1797.457153	324734.925757	37.493530
1799.200820	325373.740618	37.498548
1801.175121	326008.448558	37.503565
1804.179381	326634.271450	37.508583
1805.774723	327267.150208	37.513600
1807.140937	327897.597470	37.518618
1808.806598	328524.459718	37.523636
1810.806753	329173.500778	37.528653
1812.459913	329799.818569	37.533671
1814.646945	330444.016478	37.538688
1816.571878	331079.796356	37.543706
1818.639182	331717.348296	37.548724
1820.015961	332367.269146	37.553741
1821.650463	333000.790809	37.558759
1823.266407	333651.977599	37.563776
1825.322489	334306.942941	37.568794
1827.240413	334956.135288	37.573812
1828.760843	335614.930611	37.578829
1830.849773	336261.972221	37.583847
1832.778044	336920.303619	37.588864
1834.331341	337570.108669	37.593882
1836.259814	338237.536942	37.598900
1837.846781	338897.550101	37.603917
1839.866644	339552.330555	37.608935
1841.939485	340229.152356	37.613952
1843.677855	340870.179174	37.618970
1845.971651	341540.652083	37.623988
1847.627488	342209.469911	37.629005
1849.327738	342848.548794	37.634023
1851.633549	343514.729037	37.639040
1853.660147	344176.301483	37.644058
1854.977564	344839.377920	37.649076
1856.626380	345504.903332	37.654093
1858.980134	346166.826110	37.659111
1860.653797	346836.745134	37.664128
1862.149851	347496.049809	37.669146
1864.046102	348155.101560	37.674164
1865.750773	348834.148981	37.679181
1867.901007	349514.838693	37.684199
1869.495629	350188.224845	37.689216
1872.017213	350862.437882	37.694234
1873.687847	351506.074279	37.699252
1875.283417	352162.808505	37.704269
1877.429963	352803.454718	37.709287
1878.953215	353459.115871	37.714304
1880.835432	354107.019054	37.719322
1882.969011	354752.282823	37.724340
1884.685592	355409.938210	37.729357
1886.299788	356041.337291	37.734375
1888.144210	356709.710665	37.739392
1889.921987	357363.291330	37.744410
1892.090242	358026.946987	37.749428
1893.321539	358713.481258	37.754445
1895.264911	359375.351045	37.759463
1896.944592	360052.781746	37.764480
1899.201828	360721.352591	37.769498
1900.899479	361412.560249	37.774516
1902.722100	362110.991678	37.779533
1904.841321	362788.177363	37.784551
1906.701197	363476.582698	37.789568
1908.737029	364167.940711	37.794586
1910.931053	364862.380943	37.799604
1912.822922	365556.934787	37.804621
1914.823837	366255.339626	37.809639
1916.740578	366945.475680	37.814656
1918.741923	367648.167743	37.819674
1920.720699	368339.333829	37.824692
1922.709484	369043.879298	37.829709
1924.417205	369735.267440	37.834727
1926.445013	370437.446564	37.839744
1928.135569	371142.331389	37.844762
1930.129024	371857.501639	37.849780
1932.269788	372568.702151	37.854797
1934.370644	373273.985565	37.859815
1936.189735	373999.516301	37.864832
1937.991368	374726.354134	37.869850
1940.011525	375431.101258	37.874868
1941.661074	376164.097861	37.879885
1943.658593	376874.171303	37.884903
1945.650753	377603.556154	37.889920
1947.533031	378337.762293	37.894938
1949.376170	379062.931252	37.899956
1951.081729	379807.507369	37.904973
1953.484199	380548.072448	37.909991
1955.307841	381279.182213	37.915008
1957.087656	382023.773560	37.920026
1959.032708	382765.684001	37.925044
1960.835489	383516.501478	37.930061
1962.990523	384263.491183	37.935079
1964.876575	385018.393774	37.940096
1967.078036	385758.293054	37.945114
1968.961378	386518.206958	37.950132
1970.806426	387279.098100	37.955149
1973.087366	388030.518782	37.960167
1975.055358	388786.029760	37.965184
1976.677468	389539.551678	37.970202
1979.302913	390286.628421	37.975220
1981.303431	391037.669062	37.980237
1983.396871	391790.501482	37.985255
1985.869124	392542.239184	37.990272
1987.645164	393292.679213	37.995290
1989.689919	394041.104765	38.000308
1991.938542	394780.150499	38.005325
1994.165229	395522.933149	38.010343
1996.600131	396264.142391	38.015360
1998.122569	397005.990709	38.020378
2000.134549	397738.919830	38.025396
2001.657403	398488.207836	38.030413
2004.060748	399219.945906	38.035431
2006.500523	399958.020790	38.040448
2008.654775	400662.976357	38.045466
2010.378105	401366.338664	38.050484
2012.447923	402077.685164	38.055501
2014.431677	402774.254763	38.060519
2016.070627	403485.966804	38.065536
2017.429289	404191.220435	38.070554
2019.909688	404911.753358	38.075572
2022.102654	405629.325378	38.080589
2023.756730	406347.601331	38.085607
2025.869823	407075.791038	38.090624
2027.428106	407811.577904	38.095642
2029.425850	408533.363630	38.100660
2031.217387	409275.609406	38.105677
2033.130131	410022.552470	38.110695
2035.261875	410767.158911	38.115712
2037.005250	411523.537847	38.120730
2039.300804	412268.303842	38.125748
2041.527200	413034.465272	38.130765
2043.295914	413809.545762	38.135783
2044.936663	414562.689287	38.140800
2047.099940	415328.338905	38.145818
2049.161287	416102.012006	38.150836
2051.411933	416884.216935	38.155853
2052.886442	417664.322904	38.160871
2055.498892	418449.460108	38.165888
2057.078766	419247.026271	38.170906
2059.208319	420037.436791	38.175924
2061.452569	420843.428418	38.180941
2063.031433	421646.288161	38.185959
2065.557696	422438.305600	38.190976
2067.126662	423243.724112	38.195994
2069.773928	424060.029042	38.201012
2071.501509	424866.812124	38.206029
2073.842511	425685.899089	38.211047
2076.056342	426495.966634	38.216064
2077.969097	427317.753374	38.221082
2080.384275	428130.417015	38.226100
2082.696545	428942.462785	38.231117
2084.455549	429759.787166	38.236135
2087.122847	430583.464754	38.241152
2089.007137	431403.800525	38.246170
2091.048348	432216.741694	38.251188
2093.172582	433047.713094	38.256205
2095.319022	433875.158699	38.261223
2097.392913	434710.027842	38.266240
2099.037306	435537.851621	38.271258
2101.368260	436361.888374	38.276276
2103.305014	437203.219548	38.281293
2105.129068	438040.945111	38.286311
2107.570829	438882.434954	38.291328
2109.452023	439729.299804	38.296346
2111.438227	440572.775704	38.301364
2113.901447	441427.931849	38.306381
2116.229131	442271.338234	38.311399
2117.785701	443125.465714	38.316416
2119.535885	443987.927536	38.321434
2121.570325	444825.264138	38.326452
2123.535587	445705.635177	38.331469
2125.568870	446582.418181	38.336487
2127.842799	447452.650770	38.341504
2129.807186	448322.950037	38.346522
2132.223372	449193.999622	38.351540
2133.967221	450076.505916	38.356557
2135.743573	450974.802229	38.361575
2138.295214	451841.523289	38.366592
2140.318693	452732.825662	38.371610
2142.411187	453626.000765	38.376628
2144.406151	454509.443983	38.381645
2146.793499	455365.780534	38.386663
2149.067230	456235.551660	38.391680
2151.006086	457098.514988	38.396698
2152.779087	457947.159869	38.401716
2155.172085	458817.257298	38.406733
2157.151810	459705.283890	38.411751
2159.399040	460571.285587	38.416768
2161.363345	461437.751836	38.421786
2163.633477	462307.011881	38.426804
2165.911205	463190.134469	38.431821
2168.224635	464061.838614	38.436839
2170.833676	464936.084165	38.441856
2172.745230	465832.797158	38.446874
2175.343083	466706.915529	38.451892
2177.317058	467596.815617	38.456909
2179.389296	468478.017035	38.461927
2181.588964	469367.546289	38.466944
2183.390264	470260.637614	38.471962
2185.423034	471154.659967	38.476980
2187.877303	472065.599055	38.481997
2190.466691	472980.767059	38.487015
2192.469104	473883.205439	38.492032
2194.617246	474804.673567	38.497050
2196.053940	475711.513149	38.502068
2198.597144	476635.301793	38.507085
2200.829202	477564.046338	38.512103
2202.893630	478488.529237	38.517120
2204.543596	479434.399251	38.522138
2206.793730	480367.798421	38.527156
2208.592020	481319.607687	38.532173
2211.206221	482275.828355	38.537191
2213.650462	483243.691712	38.542208
2215.660259	484199.860154	38.547226
2218.145489	485167.310724	38.552244
2220.531039	486140.683331	38.557261
2222.366880	487109.701209	38.562279
2224.761780	488070.900563	38.567296
2227.016908	489050.950761	38.572314
2229.708728	490021.535983	38.577332
2231.747073	490982.685880	38.582349
2234.115438	491956.144826	38.587367
2236.805692	492919.553661	38.592384
2238.997380	493902.320061	38.597402
2241.557848	494868.064150	38.602420
2244.241490	495825.558882	38.607437
2246.335045	496795.913814	38.612455
2248.732539	497754.962187	38.617472
2251.199540	498710.867256	38.622490
2253.584130	499671.978631	38.627508
2255.969937	500627.435266	38.632525
2258.025457	501589.399188	38.637543
2260.309831	502555.153908	38.642560
2262.241889	503530.191259	38.647578
2264.615668	504484.722419	38.652596
2266.766521	505445.690418	38.657613
2268.911808	506424.051700	38.662631
2271.255687	507383.310889	38.667648
2273.663326	508339.729750	38.672666
2276.030172	509302.199818	38.677684
2278.486802	510290.209834	38.682701
2280.512054	511262.400161	38.687719
2282.941217	512224.685088	38.692736
2284.996236	513217.924378	38.697754
2286.931424	514175.434496	38.702772
2289.497554	515154.707600	38.707789
2291.344376	516138.271990	38.712807
2293.616697	517130.725472	38.717824
2295.724704	518106.614305	38.722842
2297.838896	519067.525707	38.727860
2300.098463	520023.012687	38.732877
2302.390548	520995.817469	38.737895
2304.255831	521962.585565	38.742912
2306.817395	522924.744774	38.747930
2309.157753	523885.469407	38.752948
2311.818661	524856.053918	38.757965
2314.056553	525831.028003	38.762983
2316.167259	526813.917647	38.768000
2318.312516	527784.499757	38.773018
2320.465194	528772.391124	38.778036
2322.732483	529770.420122	38.783053
2324.746047	530753.268453	38.788071
2326.832175	531758.645590	38.793088
2328.814252	532791.257758	38.798106
2330.880883	533797.153493	38.803124
2333.428045	534821.827570	38.808141
2335.296239	535862.849589	38.813159
2337.266831	536900.307433	38.818176
2339.554269	537952.182897	38.823194
2341.837750	539015.304783	38.828212
2344.330803	540078.615337	38.833229
2346.750767	541150.261460	38.838247
2348.946933	542210.543925	38.843264
2351.787159	543286.739279	38.848282
2353.797318	544380.947802	38.853300
2356.481287	545449.257237	38.858317
2359.090772	546531.580308	38.863335
2361.433206	547612.354790	38.868352
2363.623557	548705.843458	38.873370
2366.509414	549789.376141	38.878388
2368.704829	550890.887447	38.883405
2370.967311	551987.523261	38.888423
2373.867146	553072.655055	38.893440
2375.978753	554177.485110	38.898458
2378.319044	555273.693095	38.903476
2381.144347	556377.773837	38.908493
2383.618222	557485.993271	38.913511
2386.084225	558572.213024	38.918528
2388.470817	559678.908720	38.923546
2390.608952	560791.582600	38.928564
2393.281185	561888.501167	38.933581
2395.561178	563006.642569	38.938599
2398.169282	564106.150236	38.943616
2400.581507	565214.236916	38.948634
2403.098472	566335.872678	38.953652
2405.409843	567447.753748	38.958669
2408.206515	568568.497834	38.963687
2410.218434	569660.153005	38.968704
2412.657473	570783.073165	38.973722
2414.746985	571905.500804	38.978740
2417.240694	573025.755359	38.983757
2419.426427	574149.124101	38.988775
2421.966919	575277.052359	38.993792
2424.997536	576406.956902	38.998810
2427.059101	577540.984093	39.003828
2429.526824	578677.852109	39.008845
2432.096217	579807.526084	39.013863
2434.629635	580921.000746	39.018880
2437.325258	582057.070859	39.023898
2439.369492	583185.470126	39.028916
2441.360689	584323.654224	39.033933
2443.811897	585467.874830	39.038951
2446.575138	586608.426903	39.043968
2448.780858	587747.108893	39.048986
2450.821130	588902.906225	39.054004
2453.709887	590034.191791	39.059021
2455.800755	591177.631977	39.064039
2457.919915	592303.868491	39.069056
2460.438633	593419.910445	39.074074
2462.345120	594549.477723	39.079092
2464.895374	595674.923244	39.084109
2467.275710	596798.486022	39.089127
2469.789183	597937.047789	39.094144
2472.619839	599085.614685	39.099162
2474.407190	600222.471066	39.104180
2476.716606	601368.394950	39.109197
2479.122653	602537.323714	39.114215
2481.488336	603698.129990	39.119232
2483.601178	604858.360338	39.124250
2485.962834	606047.616369	39.129268
2488.545363	607223.498313	39.134285
2491.128765	608418.727363	39.139303
2493.299980	609623.856970	39.144320
2495.757722	610819.053695	39.149338
2497.685979	612021.465555	39.154356
2500.401184	613249.082374	39.159373
2503.175484	614479.155795	39.164391
2505.827429	615694.709176	39.169408
2508.337855	616911.803124	39.174426
2510.817444	618155.120517	39.179444
2513.124928	619409.025711	39.184461
2515.919519	620644.809959	39.189479
2518.522929	621881.835756	39.194496
2521.551769	623128.747283	39.199514
2523.455283	624382.497804	39.204532
2526.147554	625628.777344	39.209549
2528.706896	626898.567716	39.214567
2531.117161	628168.831998	39.219584
2533.618095	629432.786376	39.224602
2535.946560	630715.299197	39.229620
2538.611112	631994.305663	39.234637
2541.127201	633272.682614	39.239655
2543.201057	634565.256828	39.244672
2546.079491	635853.146187	39.249690
2548.281272	637157.460694	39.254708
2550.439429	638466.660015	39.259725
2553.218696	639780.083158	39.264743
2555.738608	641090.637946	39.269760
2558.637632	642410.243173	39.274778
2560.844630	643740.617639	39.279796
2563.461232	645066.112954	39.284813
2566.112574	646394.522102	39.289831
2568.657374	647739.329907	39.294848
2571.547602	649056.230933	39.299866
2574.212117	650391.242549	39.304884
2576.749564	651737.262706	39.309901
2579.588263	653080.659823	39.314919
2582.190428	654413.948567	39.319936
2585.276329	655743.341303	39.324954
2587.636790	657078.005372	39.329972
2590.642666	658407.401187	39.334989
2593.304165	659735.030186	39.340007
2595.842148	661069.719953	39.345024
2598.735110	662378.177742	39.350042
2600.957020	663725.998598	39.355060
2603.606527	665063.257432	39.360077
2606.543820	666387.890609	39.365095
2609.043290	667714.254497	39.370112
2611.814243	669041.185931	39.375130
2614.535209	670377.293824	39.380148
2617.443417	671697.762896	39.385165
2619.758988	673022.522204	39.390183
2621.794147	674354.053979	39.395200
2624.689499	675688.288418	39.400218
2627.401303	677009.238550	39.405236
2630.247050	678312.433062	39.410253
2632.670666	679594.441664	39.415271
2635.002072	680890.848399	39.420288
2637.683467	682188.009308	39.425306
2640.231997	683483.469339	39.430324
2642.617637	684777.283195	39.435341
2645.617890	686071.657062	39.440359
2647.903026	687368.994150	39.445376
2650.580212	688671.543013	39.450394
2653.028590	690004.820735	39.455412
2655.437241	691318.549761	39.460429
2658.065387	692637.758077	39.465447
2660.386131	693981.336119	39.470464
2663.124523	695334.069956	39.475482
2665.481687	696682.345243	39.480500
2667.981699	698042.891066	39.485517
2670.380209	699399.921578	39.490535
2672.566412	700783.553317	39.495552
2675.518421	702154.992110	39.500570
2678.261249	703544.094896	39.505588
2681.007740	704932.133190	39.510605
2684.062404	706315.835603	39.515623
2687.027805	707709.141307	39.520640
2690.556924	709098.810104	39.525658
2693.833485	710481.807618	39.530676
2696.247141	711859.276807	39.535693
2699.969588	713233.634378	39.540711
2702.439199	714609.461503	39.545728
2705.460905	715977.896425	39.550746
2708.076579	717357.558957	39.555764
2710.628534	718745.566037	39.560781
2713.389039	720128.015712	39.565799
2715.325870	721523.529998	39.570816
2717.628955	722904.358812	39.575834
2720.554256	724322.583752	39.580852
2723.045028	725737.522728	39.585869
2725.698682	727145.024858	39.590887
2728.104910	728581.436133	39.595904
2730.516053	730005.291023	39.600922
2733.411621	731447.986641	39.605940
2735.731219	732891.904473	39.610957
2738.221606	734352.130941	39.615975
2740.864719	735805.402429	39.620992
2743.919909	737270.636520	39.626010
2746.392971	738744.583706	39.631028
2749.273471	740207.828503	39.636045
2752.519976	741679.675067	39.641063
2754.471462	743165.373875	39.646080
2757.158220	744645.345758	39.651098
2759.974781	746128.618377	39.656116
2762.627735	747631.606146	39.661133
2765.300661	749130.900817	39.666151
2767.856530	750630.025272	39.671168
2770.860604	752141.697039	39.676186
2774.229160	753649.269587	39.681204
2777.363675	755142.991557	39.686221
2780.465691	756642.239991	39.691239
2783.028618	758138.526812	39.696256
2786.263852	759622.595232	39.701274
2788.895798	761123.158670	39.706292
2791.495599	762625.595843	39.711309
2794.164510	764121.671746	39.716327
2796.752418	765624.301213	39.721344
2799.490427	767136.391863	39.726362
2802.646765	768645.551318	39.731380
2805.107573	770149.751620	39.736397
2808.200419	771656.443167	39.741415
2811.040759	773156.530956	39.746432
2813.723393	774634.182812	39.751450
2816.319766	776101.973918	39.756468
2818.977423	777567.644116	39.761485
2822.183538	779025.614222	39.766503
2825.300729	780496.463187	39.771520
2828.176972	781949.974188	39.776538
2831.241758	783402.033601	39.781556
2833.545573	784874.972820	39.786573
2836.113447	786348.008281	39.791591
2838.567746	787837.923577	39.796608
2841.361933	789318.009468	39.801626
2844.246564	790815.174551	39.806644
2846.899661	792306.180873	39.811661
2849.833392	793805.695350	39.816679
2852.826568	795325.896832	39.821696
2855.144737	796839.562567	39.826714
2857.952757	798350.029338	39.831732
2860.264468	799891.533809	39.836749
2863.529864	801425.736216	39.841767
2866.059324	802981.642792	39.846784
2868.624426	804538.073760	39.851802
2871.302690	806102.693869	39.856820
2874.178023	807679.345540	39.861837
2876.598034	809263.042156	39.866855
2879.311686	810866.166795	39.871872
2882.174089	812467.129387	39.876890
2885.031871	814086.425351	39.881908
2887.627717	815711.236872	39.886925
2890.630773	817325.968892	39.891943
2893.174341	818963.576408	39.896960
2896.403541	820600.425191	39.901978
2899.722197	822243.590121	39.906996
2902.436479	823906.643311	39.912013
2905.480293	825556.299363	39.917031
2908.398048	827208.878286	39.922048
2911.100942	828866.779504	39.927066
2914.455614	830526.102151	39.932084
2917.434881	832199.144233	39.937101
2920.339366	833864.363711	39.942119
2923.447379	835539.590494	39.947136
2926.590250	837211.552466	39.952154
2929.867012	838870.646141	39.957172
2932.263110	840557.287018	39.962189
2935.304662	842213.118455	39.967207
2938.225298	843889.401608	39.972224
2941.244866	845570.670148	39.977242
2944.133126	847259.192222	39.982260
2946.898473	848949.710883	39.987277
2950.026521	850623.390931	39.992295
2952.941013	852318.707030	39.997312
2955.616167	854011.949960	40.002330
2959.021139	855713.541808	40.007348
2961.637625	857410.718804	40.012365
2964.523266	859113.496508	40.017383
2967.067799	860827.886000	40.022400
2970.089348	862546.758947	40.027418
2973.277630	864262.889905	40.032436
2975.730878	865993.000836	40.037453
2978.649102	867710.429378	40.042471
2981.750196	869449.132698	40.047488
2984.583261	871186.892964	40.052506
2987.918254	872909.061365	40.057524
2990.617490	874651.451183	40.062541
2993.791257	876379.126908	40.067559
2996.758943	878121.904993	40.072576
2999.996473	879856.678964	40.077594
3003.305417	881597.889554	40.082612
3006.077681	883316.445400	40.087629
3009.317939	885000.992626	40.092647
3012.526232	886697.033737	40.097664
3015.048295	888377.051006	40.102682
3018.342629	890059.445414	40.107700
3021.082198	891748.773916	40.112717
3024.076558	893428.881829	40.117735
3027.157774	895121.308862	40.122752
3029.932148	896819.744081	40.127770
3033.144118	898503.335794	40.132788
3036.000502	900226.761261	40.137805
3038.738122	901927.237580	40.142823
3041.608128	903651.733435	40.147840
3044.345452	905375.336269	40.152858
3047.593748	907105.733839	40.157876
3050.130374	908848.314195	40.162893
3053.336655	910589.275977	40.167911
3056.334763	912343.184627	40.172928
3058.814984	914116.900739	40.177946
3062.274009	915888.250149	40.182964
3064.779767	917680.122784	40.187981
3068.237464	919453.775422	40.192999
3071.425404	921239.948576	40.198016
3074.290985	923041.515017	40.203034
3077.433526	924845.984421	40.208052
3080.506513	926653.792169	40.213069
3083.780265	928450.125920	40.218087
3086.689167	930272.172607	40.223104
3089.572361	932109.214773	40.228122
3093.015538	933928.196811	40.233140
3096.187098	935754.639344	40.238157
3099.210984	937594.062014	40.243175
3102.326542	939432.730059	40.248192
3105.069439	941276.647044	40.253210
3108.515127	943126.105736	40.258228
3111.160330	944985.167514	40.263245
3114.052642	946847.533546	40.268263
3117.308354	948720.626529	40.273280
3119.935034	950611.372705	40.278298
3123.646048	952480.155502	40.283316
3126.542757	954373.188243	40.288333
3129.157178	956302.092887	40.293351
3132.067721	958258.408050	40.298368
3134.628308	960224.188090	40.303386
3137.742759	962189.890927	40.308404
3141.279090	964178.106938	40.313421
3144.435876	966161.694184	40.318439
3147.414146	968147.946224	40.323456
3150.608336	970140.600957	40.328474
3153.570351	972145.578702	40.333492
3156.334691	974149.985584	40.338509
3159.034671	976157.601861	40.343527
3162.480623	978192.363632	40.348544
3165.285610	980218.615150	40.353562
3168.548061	982249.721695	40.358580
3171.352352	984293.908859	40.363597
3174.613761	986329.501944	40.368615
3177.954133	988381.088778	40.373632
3181.126104	990441.786706	40.378650
3184.489420	992490.526010	40.383668
3187.289107	994569.427059	40.388685
3190.329847	996610.221506	40.393703
3193.651345	998678.495639	40.398720
3196.459324	1000767.068280	40.403738
3200.057027	1002837.660528	40.408756
3203.005121	1004920.406461	40.413773
3206.232954	1006997.683750	40.418791
3209.536525	1009078.933762	40.423808
3212.455214	1011152.598912	40.428826
3216.064142	1013186.834644	40.433844
3219.188546	1015236.101195	40.438861
3222.597886	1017265.892352	40.443879
3226.039870	1019279.946655	40.448896
3228.879091	1021322.298123	40.453914
3231.993183	1023340.557918	40.458932
3235.172474	1025372.577897	40.463949
3238.047265	1027416.180741	40.468967
3241.899558	1029463.897817	40.473984
3245.316394	1031508.232265	40.479002
3248.363709	1033545.025932	40.484020
3251.355016	1035602.309726	40.489037
3254.163726	1037667.253986	40.494055
3257.336990	1039736.192025	40.499072
3260.961734	1041815.946264	40.504090
3264.070232	1043895.680736	40.509108
3267.247928	1045997.157691	40.514125
3270.335499	1048104.013191	40.519143
3273.590053	1050194.932039	40.524160
3276.214511	1052319.407013	40.529178
3279.747499	1054432.627274	40.534196
3282.924865	1056572.201015	40.539213
3286.174928	1058699.883685	40.544231
3289.946658	1060840.392098	40.549248
3292.827554	1062995.190716	40.554266
3296.495892	1065136.923467	40.559284
3299.969828	1067287.541389	40.564301
3303.304677	1069450.571654	40.569319
3306.799682	1071613.296807	40.574336
3309.558557	1073780.654238	40.579354
3313.118907	1075945.105203	40.584372
3316.211390	1078121.029907	40.589389
3319.875158	1080298.002586	40.594407
3323.898867	1082473.568266	40.599424
3327.129368	1084656.045123	40.604442
3330.213369	1086822.663888	40.609460
3333.746646	1089002.485618	40.614477
3336.968568	1091197.146464	40.619495
3340.357611	1093380.676517	40.624512
3343.423075	1095591.340628	40.629530
3346.681111	1097787.524526	40.634548
3349.706828	1099984.380096	40.639565
3353.011107	1102199.835245	40.644583
3356.358145	1104417.517496	40.649600
3359.471038	1106634.706555	40.654618
3362.985020	1108855.104898	40.659636
3366.271426	1111096.033793	40.664653
3369.720008	1113319.355792	40.669671
3373.424639	1115546.563203	40.674688
3376.489038	1117783.594614	40.679706
3380.026121	1120011.633744	40.684724
3383.262377	1122245.915985	40.689741
3386.717464	1124499.729937	40.694759
3390.532493	1126743.898867	40.699776
3393.649509	1128995.962941	40.704794
3397.264727	1131223.293149	40.709812
3400.633941	1133465.081884	40.714829
3403.451263	1135715.392662	40.719847
3407.349458	1137960.405549	40.724864
3410.369202	1140213.886790	40.729882
3413.603499	1142462.116941	40.734900
3417.133975	1144723.999069	40.739917
3420.387303	1146992.992431	40.744935
3423.859388	1149240.945583	40.749952
3427.135021	1151514.981010	40.754970
3430.491935	1153774.994738	40.759988
3433.910688	1156047.519888	40.765005
3437.262678	1158287.471383	40.770010
3441.035654	1160482.322070	40.775015
3443.972742	1162626.602843	40.780020
3447.357514	1164693.625982	40.785024
3450.889240	1166684.380878	40.790029
3453.707461	1168597.679727	40.795034
3456.735532	1170438.171483	40.800039
3459.983278	1172201.781324	40.805044
3462.707578	1173870.419937	40.810048
3466.064294	1175479.988897	40.815053
3468.799912	1176996.265714	40.820058
3471.865179	1178421.812325	40.825063
3474.215171	1179779.569044	40.830068
3476.412655	1181054.056706	40.835072
3478.976727	1182253.157048	40.840077
3480.679043	1183395.285742	40.845082
3482.931729	1184455.128193	40.850087
3485.224412	1185458.686050	40.855092
3486.495555	1186396.009783	40.860096
3488.507027	1187265.246673	40.865101
3490.335040	1188085.292046	40.870106
3492.187363	1188843.350868	40.875111
3493.672621	1189562.729929	40.880116
3494.951131	1190212.218899	40.885120
3496.586672	1190816.840071	40.890125
3497.611358	1191375.829001	40.895130
3498.812192	1191885.219128	40.900135
3500.264680	1192362.485025	40.905140
3501.412537	1192788.565621	40.910144
3502.782236	1193179.917253	40.915149
3503.292433	1193534.190166	40.920154
3504.516444	1193853.105030	40.925159
3505.380018	1194134.685485	40.930164
3506.370732	1194386.275489	40.935168
3507.411424	1194602.727839	40.940173
3508.192172	1194789.919370	40.945178
3508.848381	1194934.123002	40.950183
3509.164464	1195072.369790	40.955188
3509.735685	1195165.036272	40.960192
3510.603699	1195247.512676	40.965197
3511.009148	1195320.393962	40.970202
3511.878451	1195362.310560	40.975207
3512.226149	1195384.597506	40.980212
3512.772511	1195385.352678	40.985216
3513.232385	1195371.851993	40.990221
3513.790620	1195341.530060	40.995226
3514.430235	1195287.066441	41.000231
3515.152101	1195228.739420	41.005236
3515.297683	1195135.111495	41.010240
3515.611614	1195036.759724	41.015245
3515.878319	1194931.747643	41.020250
3516.284800	1194799.199892	41.025255
3516.535787	1194666.298763	41.030260
3516.865113	1194505.024147	41.035264
3517.148162	1194352.015398	41.040269
3517.131550	1194185.059789	41.045274
3517.446884	1193999.168763	41.050279
3517.524118	1193822.889138	41.055284
3517.303154	1193628.808948	41.060288
3517.846698	1193424.076763	41.065293
3518.237294	1193235.422208	41.070298
3518.208247	1193013.674344	41.075303
3518.885934	1192794.524510	41.080308
3519.016813	1192561.835085	41.085312
3518.887082	1192322.790318	41.090317
3518.583653	1192073.993081	41.095322
3518.906797	1191824.235137	41.100327
3519.202841	1191589.032037	41.105332
3519.338412	1191328.288693	41.110336
3519.327779	1191059.005830	41.115341
3519.581158	1190798.122359	41.120346
3519.610544	1190526.455999	41.125351
3519.808711	1190244.504217	41.130356
3519.760939	1189972.257567	41.135360
3520.437604	1189697.057699	41.140365
3519.958281	1189408.780863	41.145370
3520.127476	1189110.511536	41.150375
3520.290971	1188821.532101	41.155380
3519.787862	1188523.809649	41.160384
3520.346444	1188223.638901	41.165389
3520.440158	1187937.629960	41.170394
3520.577458	1187608.817464	41.175399
3520.525015	1187306.343534	41.180404
3520.651983	1186991.221721	41.185408
3520.739262	1186680.601200	41.190413
3520.525960	1186361.359289	41.195418
3520.822067	1186039.662490	41.200423
3521.072119	1185716.730537	41.205428
3521.025758	1185393.262880	41.210432
3521.065117	1185066.562529	41.215437
3520.877204	1184742.889422	41.220442
3521.077554	1184407.560103	41.225447
3521.033785	1184082.128503	41.230452
3520.889548	1183758.386695	41.235456
3520.947337	1183409.654983	41.240461
3520.635981	1183082.887305	41.245466
3520.819391	1182749.335606	41.250471
3520.979048	1182417.084017	41.255476
3520.856004	1182075.633551	41.260480
3521.032050	1181742.112418	41.265485
3520.764852	1181403.747760	41.270490
3521.027561	1181066.874184	41.275495
3521.009865	1180732.378638	41.280500
3520.966217	1180394.005473	41.285504
3521.065746	1180046.829718	41.290509
3521.181780	1179703.771388	41.295514
3521.133455	1179352.524381	41.300519
3521.063987	1179012.370313	41.305524
3520.646558	1178663.397801	41.310528
3521.092302	1178321.795068	41.315533
3521.343128	1177974.455888	41.320538
3520.901708	1177613.076775	41.325543
3520.472006	1177269.288132	41.330548
3520.774150	1176924.696701	41.335552
3521.048215	1176576.506565	41.340557
3520.786805	1176231.019754	41.345562
3520.800767	1175877.360315	41.350567
3520.852017	1175530.361935	41.355572
3520.784359	1175182.888757	41.360576
3520.695053	1174829.929135	41.365581
3520.429354	1174476.220535	41.370586
3520.660039	1174135.509419	41.375591
3520.752309	1173795.081635	41.380596
3520.314826	1173438.879731	41.385600
3520.643379	1173097.141775	41.390605
3520.465677	1172748.204224	41.395610
3520.477209	1172393.648472	41.400615
3520.600104	1172047.726400	41.405620
3520.373834	1171706.931725	41.410624
3520.598926	1171350.477929	41.415629
3520.055920	1171023.272555	41.420634
3520.337119	1170654.782775	41.425639
3520.229698	1170310.953032	41.430644
3520.360803	1169969.608618	41.435648
3520.886581	1169618.647572	41.440653
3520.716226	1169264.475120	41.445658
3520.498599	1168902.737417	41.450663
3520.571023	1168549.514465	41.455668
3520.440528	1168194.507909	41.460672
3520.344901	1167842.302932	41.465677
3520.172278	1167493.862411	41.470682
3520.294737	1167138.459260	41.475687
3520.232059	1166789.670490	41.480692
3519.909362	1166441.845336	41.485696
3520.162172	1166096.734653	41.490701
3519.820557	1165749.433021	41.495706
3519.985679	1165393.526529	41.500711
3519.834453	1165055.212324	41.505716
3519.921167	1164713.720588	41.510720
3520.220060	1164354.416036	41.515725
3520.112659	1164016.783023	41.520730
3519.962090	1163663.077631	41.525735
3519.760841	1163309.262218	41.530740
3519.670279	1162966.079762	41.535744
3519.898595	1162628.301904	41.540749
3519.772455	1162276.199357	41.545754
3519.877399	1161917.231900	41.550759
3519.820525	1161583.874638	41.555764
3519.965778	1161236.476750	41.560768
3519.801959	1160876.348242	41.565773
3519.538754	1160535.586689	41.570778
3519.380825	1160193.367848	41.575783
3519.675856	1159845.475036	41.580788
3519.500165	1159497.447612	41.585792
3519.744809	1159149.327870	41.590797
3519.409531	1158805.535059	41.595802
3519.075099	1158466.352574	41.600807
3519.388540	1158121.651711	41.605812
3518.919015	1157783.298341	41.610816
3519.096953	1157440.371764	41.615821
3518.871042	1157104.960771	41.620826
3519.179211	1156767.265020	41.625831
3518.896937	1156430.212330	41.630836
3519.010843	1156087.775515	41.635840
3519.256291	1155746.619121	41.640845
3518.631439	1155413.909238	41.645850
3519.103482	1155073.334069	41.650855
3518.827625	1154734.090051	41.655860
3518.570048	1154398.889970	41.660864
3518.825232	1154060.650534	41.665869
3518.611125	1153733.539078	41.670874
3518.756172	1153404.455288	41.675879
3518.806729	1153067.037451	41.680884
3518.495071	1152735.904805	41.685888
3518.977177	1152404.620595	41.690893
3518.374026	1152066.204989	41.695898
3518.676026	1151731.310765	41.700903
3518.616654	1151408.952263	41.705908
3518.181704	1151067.320367	41.710912
3518.869245	1150732.677894	41.715917
3518.070802	1150400.910394	41.720922
3518.525832	1150060.581771	41.725927
3518.047038	1149736.958893	41.730932
3518.286982	1149403.158094	41.735936
3518.266965	1149068.621219	41.740941
3518.375948	1148750.334718	41.745946
3518.302991	1148421.733237	41.750951
3518.454443	1148090.800624	41.755956
3518.201044	1147758.777005	41.760960
3518.226692	1147421.475307	41.765965
3517.707165	1147107.551665	41.770970
3517.891903	1146783.448697	41.775975
3517.891221	1146445.141324	41.780980
3517.937549	1146130.497769	41.785984
3518.077330	1145800.560732	41.790989
3517.793256	1145486.881029	41.795994
3517.725914	1145173.336578	41.800999
3518.016701	1144850.519360	41.806004
3517.551344	1144529.134173	41.811008
3517.909469	1144187.399831	41.816013
3517.550585	1143872.878143	41.821018
3517.820049	1143549.321269	41.826023
3517.660927	1143226.289306	41.831028
3517.517024	1142900.485010	41.836032
3517.673501	1142571.102218	41.841037
3517.736435	1142258.785946	41.846042
3517.450334	1141946.224176	41.851047
3517.846019	1141621.200697	41.856052
3517.314302	1141303.519310	41.861056
3517.441978	1140985.710250	41.866061
3517.149970	1140670.322996	41.871066
3517.051616	1140348.148834	41.876071
3517.238879	1140042.797035	41.881076
3516.976624	1139736.647680	41.886080
3517.421814	1139412.524224	41.891085
3517.369421	1139106.114079	41.896090
3517.066116	1138795.741558	41.901095
3516.903413	1138480.107656	41.906100
3516.390462	1138175.238083	41.911104
3516.755333	1137857.961598	41.916109
3517.112275	1137560.222306	41.921114
3516.661009	1137251.872113	41.926119
3516.614585	1136937.076501	41.931124
3516.936131	1136628.183018	41.936128
3516.673997	1136320.222219	41.941133
3516.553729	1136013.264670	41.946138
3516.502996	1135711.215806	41.951143
3516.850471	1135405.570468	41.956148
3516.788599	1135099.785012	41.961152
3516.329604	1134799.555941	41.966157
3516.488312	1134491.989585	41.971162
3516.563625	1134176.630232	41.976167
3516.759922	1133888.020061	41.981172
3516.418490	1133587.988095	41.986176
3516.843656	1133271.947437	41.991181
3516.483311	1132974.068984	41.996186
3516.544539	1132674.489165	42.001191
3516.527509	1132362.932928	42.006196
3516.435345	1132064.769298	42.011200
3516.371683	1131750.904281	42.016205
3516.486888	1131448.395573	42.021210
3516.649357	1131132.841232	42.026215
3516.283800	1130839.596074	42.031220
3516.014614	1130540.045453	42.036224
3516.226048	1130236.026173	42.041229
3516.051043	1129945.266879	42.046234
3515.894675	1129646.883204	42.051239
3516.327984	1129352.854125	42.056244
3516.060798	1129056.166906	42.061248
3516.053236	1128749.246428	42.066253
3515.618522	1128457.402706	42.071258
3515.847420	1128157.350673	42.076263
3515.835616	1127876.816808	42.081268
3515.843569	1127574.200636	42.086272
3515.984805	1127272.496429	42.091277
3515.707883	1126992.530331	42.096282
3515.812057	1126690.704179	42.101287
3515.902174	1126399.707610	42.106292
3515.107325	1126104.845401	42.111296
3515.452468	1125807.305581	42.116301
3515.791169	1125531.632773	42.121306
3515.573348	1125241.955717	42.126311
3515.601971	1124947.940514	42.131316
3515.232978	1124657.305086	42.136320
3515.671048	1124374.704838	42.141325
3515.423962	1124084.874610	42.146330
3515.430792	1123792.797858	42.151335
3515.258334	1123512.917362	42.156340
3514.952386	1123228.189877	42.161344
3515.052025	1122948.615715	42.166349
3514.922570	1122666.399262	42.171354
3514.980202	1122384.708268	42.176359
3515.088475	1122100.233210	42.181364
3514.717473	1121831.626368	42.186368
3514.869138	1121547.495564	42.191373
3514.707458	1121278.445588	42.196378
3515.010204	1120993.117829	42.201383
3515.156722	1120713.514208	42.206388
3514.619869	1120433.151423	42.211392
3514.933982	1120154.157576	42.216397
3514.790488	1119890.272775	42.221402
3514.739104	1119600.357413	42.226407
3514.921289	1119324.294669	42.231412
3514.496508	1119051.461120	42.236416
3514.739907	1118781.456717	42.241421
3514.542350	1118514.750374	42.246426
3514.546829	1118229.514841	42.251431
3514.754018	1117958.426901	42.256436
3514.230142	1117684.587206	42.261440
3514.760063	1117405.128640	42.266445
3514.701956	1117131.946258	42.271450
3514.698294	1116864.935196	42.276455
3514.711575	1116585.995465	42.281460
3514.559927	1116305.352871	42.286464
3514.328355	1116031.952341	42.291469
3514.432076	1115773.351815	42.296474
3514.131281	1115498.505737	42.301479
3514.478857	1115223.443455	42.306484
3514.183541	1114958.291901	42.311488
3514.492301	1114699.510472	42.316493
3513.813156	1114425.052994	42.321498
3513.879382	1114154.558490	42.326503
3514.177659	1113899.553945	42.331508
3513.916266	1113634.045265	42.336512
3514.223751	1113369.669403	42.341517
3514.212068	1113112.199182	42.346522
3514.146424	1112836.701102	42.351527
3513.898206	1112573.808063	42.356532
3514.047028	1112316.559352	42.361536
3513.982672	1112041.401742	42.366541
3513.834434	1111790.281146	42.371546
3513.734160	1111521.779828	42.376551
3513.877084	1111251.221727	42.381556
3513.587262	1111007.528683	42.386560
3513.535172	1110743.559710	42.391565
3513.705936	1110485.456430	42.396570
3513.307270	1110220.850988	42.401575
3513.299019	1109974.870201	42.406580
3513.410843	1109717.407665	42.411584
3513.710463	1109464.291524	42.416589
3513.369752	1109212.318675	42.421594
3512.919923	1108958.825003	42.426599
3513.041937	1108712.096920	42.431604
3513.164625	1108468.602536	42.436608
3513.196575	1108223.871232	42.441613
3513.125751	1107976.186659	42.446618
3512.939521	1107722.113996	42.451623
3513.130832	1107463.957721	42.456628
3513.086960	1107225.494022	42.461632
3513.312585	1106974.564104	42.466637
3513.226278	1106727.110993	42.471642
3512.912636	1106487.131393	42.476647
3512.945062	1106241.355035	42.481652
3512.699128	1105998.573453	42.486656
3512.636324	1105758.042591	42.491661
3512.834419	1105517.744509	42.496666
3512.600459	1105271.872274	42.501671
3512.762719	1105033.850546	42.506676
3512.620163	1104804.559910	42.511680
3512.645326	1104556.702155	42.516685
3512.713382	1104319.428497	42.521690
3512.573527	1104079.503998	42.526695
3512.655977	1103839.723259	42.531700
3512.423377	1103601.607771	42.536704
3512.555574	1103359.409194	42.541709
3512.261648	1103126.537268	42.546714
3512.406446	1102895.016182	42.551719
3512.316413	1102651.580343	42.556724
3512.341108	1102417.192085	42.561728
3512.431014	1102185.745147	42.566733
3512.319781	1101957.092658	42.571738
3512.389106	1101713.970498	42.576743
3512.090959	1101477.683296	42.581748
3511.761947	1101260.027531	42.586752
3511.977116	1101036.060882	42.591757
3511.999237	1100812.116736	42.596762
3511.927821	1100584.642075	42.601767
3511.890179	1100349.505168	42.606772
3511.962657	1100136.612997	42.611776
3512.341517	1099895.269790	42.616781
3512.068526	1099667.980901	42.621786
3512.036588	1099447.430687	42.626791
3512.397486	1099216.289806	42.631796
3511.885992	1098986.908137	42.636800
3512.025034	1098753.967372	42.641805
3512.147772	1098526.756518	42.646810
3511.829360	1098302.860019	42.651815
3511.654852	1098067.359421	42.656820
3511.957275	1097837.794911	42.661824
3511.731392	1097622.557604	42.666829
3511.795551	1097401.334221	42.671834
3511.730191	1097183.661978	42.676839
3511.994845	1096956.361745	42.681844
3511.378034	1096731.492803	42.686848
3511.550793	1096502.753850	42.691853
3511.808550	1096283.939953	42.696858
3511.332096	1096062.655184	42.701863
3511.395806	1095839.167688	42.706868
3510.891148	1095629.541398	42.711872
3511.260339	1095417.562515	42.716877
3511.207530	1095205.740515	42.721882
3511.129271	1094994.201467	42.726887
3511.329621	1094783.852200	42.731892
3510.816479	1094570.071704	42.736896
3510.933870	1094352.925291	42.741901
3511.048443	1094148.881342	42.746906
3510.771828	1093947.382386	42.751911
3511.307743	1093732.726136	42.756916
3511.447511	1093526.166230	42.761920
3511.214319	1093300.421502	42.766925
3511.231596	1093104.107008	42.771930
3510.842981	1092889.761064	42.776935
3511.162607	1092675.672892	42.781940
3510.931076	1092471.622770	42.786945
3510.840919	1092262.084969	42.791949
3510.947454	1092054.517119	42.796954
3510.323732	1091845.051068	42.801959
3510.825007	1091645.253143	42.806964
3510.485805	1091437.830834	42.811969
3510.679330	1091241.419840	42.816973
3510.714447	1091035.739747	42.821978
3510.354479	1090831.649035	42.826983
3510.657709	1090621.791533	42.831988
3510.741794	1090435.807307	42.836993
3510.684224	1090219.098637	42.841997
3510.938177	1090018.802712	42.847002
3510.346519	1089829.461220	42.852007
3510.691006	1089624.155530	42.857012
3510.491069	1089424.582876	42.862017
3510.982639	1089217.896655	42.867021
3510.733619	1089026.938155	42.872026
3510.312897	1088813.489982	42.877031
3510.465628	1088610.189177	42.882036
3510.283112	1088412.683963	42.887041
3510.455074	1088214.921578	42.892045
3510.058853	1088019.640736	42.897050
3510.196550	1087829.630300	42.902055
3510.314384	1087634.059312	42.907060
3510.009697	1087435.197277	42.912065
3510.212807	1087248.796800	42.917069
3510.143093	1087055.727209	42.922074
3510.080014	1086862.745491	42.927079
3510.154209	1086669.830143	42.932084
3510.105477	1086480.953214	42.937089
3509.866856	1086286.350764	42.942093
3510.121126	1086098.656533	42.947098
3509.899209	1085905.571147	42.952103
3510.147428	1085707.417408	42.957108
3509.782901	1085528.239969	42.962113
3509.698087	1085334.824179	42.967117
3509.815404	1085147.886521	42.972122
3509.828494	1084975.913838	42.977127
3509.802084	1084788.220608	42.982132
3510.062110	1084597.693585	42.987137
3509.907845	1084406.461161	42.992141
3509.910384	1084224.304188	42.997146
3509.696350	1084047.737636	43.002151
3509.721029	1083851.662402	43.007156
3509.636915	1083663.076938	43.012161
3509.610547	1083485.790059	43.017165
3509.715252	1083302.914212	43.022170
3509.469006	1083128.049138	43.027175
3509.708697	1082943.796497	43.032180
3509.537167	1082761.715134	43.037185
3509.785603	1082582.531494	43.042189
3509.353852	1082400.864530	43.047194
3509.277110	1082210.597134	43.052199
3509.447447	1082033.614206	43.057204
3509.328111	1081867.319824	43.062209
3509.386141	1081686.795267	43.067213
3509.654112	1081502.872900	43.072218
3509.246510	1081335.650547	43.077223
3509.165191	1081149.375662	43.082228
3509.573445	1080975.676659	43.087233
3509.325368	1080799.010333	43.092237
3509.224206	1080617.613167	43.097242
3508.731959	1080451.720738	43.102247
3508.959300	1080275.055066	43.107252
3508.884651	1080104.190178	43.112257
3508.916167	1079934.070044	43.117261
3508.880358	1079765.203068	43.122266
3509.347604	1079601.237673	43.127271
3509.463742	1079420.340609	43.132276
3509.200352	1079262.626689	43.137281
3508.847848	1079079.972259	43.142285
3508.800083	1078913.192080	43.147290
3508.747686	1078754.085162	43.152295
3508.819252	1078575.950561	43.157300
3508.736889	1078410.888238	43.162305
3508.852028	1078240.989450	43.167309
3509.153082	1078071.054754	43.172314
3508.672515	1077914.297428	43.177319
3508.867624	1077754.736667	43.182324
3508.662455	1077589.285767	43.187329
3508.837070	1077413.016043	43.192333
3508.961374	1077242.316714	43.197338
3508.419613	1077091.593602	43.202343
3508.931538	1076908.340092	43.207348
3508.598009	1076747.972952	43.212353
3508.539752	1076591.204066	43.217357
3508.939954	1076426.098249	43.222362
3508.967540	1076252.119528	43.227367
3509.057380	1076078.028997	43.232372
3509.094260	1075914.503831	43.237377
3508.855344	1075749.482829	43.242381
3508.770579	1075587.408246	43.247386
3508.375627	1075415.104891	43.252391
3509.025114	1075250.114546	43.257396
3508.504763	1075083.967412	43.262401
3508.686713	1074921.445010	43.267405
3508.519441	1074766.946618	43.272410
3508.474400	1074604.548219	43.277415
3508.787097	1074434.306371	43.282420
3508.462567	1074278.955671	43.287425
3508.265003	1074113.110042	43.292429
3508.381873	1073958.253839	43.297434
3508.286899	1073799.874034	43.302439
3508.896399	1073640.509080	43.307444
3508.765124	1073475.305607	43.312449
3508.199583	1073307.959156	43.317453
3508.655308	1073163.399719	43.322458
3508.205143	1072999.195063	43.327463
3508.798768	1072826.262981	43.332468
3508.658719	1072673.045967	43.337473
3508.665280	1072502.794425	43.342477
3508.645649	1072341.477587	43.347482
3507.955245	1072204.672109	43.352487
3508.683042	1072039.764219	43.357492
3508.442628	1071868.188379	43.362497
3508.405417	1071719.443993	43.367501
3508.395404	1071557.621999	43.372506
3507.889131	1071403.853179	43.377511
3508.161891	1071245.050541	43.382516
3507.836608	1071100.661365	43.387521
3508.239950	1070954.995094	43.392525
3508.270744	1070787.281084	43.397530
3507.923182	1070645.574649	43.402535
3507.787795	1070485.952211	43.407540
3508.234615	1070348.336318	43.412545
3507.879585	1070193.739649	43.417549
3508.030059	1070040.304958	43.422554
3507.927718	1069899.307806	43.427559
3507.941239	1069739.446837	43.432564
3507.832779	1069595.943549	43.437569
3507.741741	1069439.455623	43.442573
3508.103463	1069292.406142	43.447578
3507.602722	1069160.684652	43.452583
3507.675954	1069003.580394	43.457588
3508.072370	1068857.282659	43.462593
3507.867384	1068708.580266	43.467597
3507.553886	1068564.987602	43.472602
3507.552315	1068425.378156	43.477607
3507.726295	1068276.890091	43.482612
3507.735917	1068132.752117	43.487617
3507.698291	1067981.694685	43.492621
3507.908964	1067847.612799	43.497626
3507.595964	1067702.939692	43.502631
3507.586961	1067549.076874	43.507636
3507.541543	1067424.547315	43.512641
3507.557363	1067274.615631	43.517645
3507.566774	1067131.124566	43.522650
3507.014521	1067003.206649	43.527655
3507.479337	1066852.708605	43.532660
3507.393083	1066723.649450	43.537665
3507.493787	1066592.632800	43.542669
3507.439833	1066453.558887	43.547674
3507.124525	1066319.911035	43.552679
3507.532593	1066168.056935	43.557684
3507.507732	1066038.875372	43.562689
3507.110624	1065889.166222	43.567693
3507.239219	1065758.413652	43.572698
3507.309927	1065633.920522	43.577703
3507.436226	1065484.402727	43.582708
3507.376640	1065350.592947	43.587713
3506.820532	1065214.456492	43.592717
3507.222865	1065071.616522	43.597722
3507.415726	1064950.455131	43.602727
3507.259889	1064821.170272	43.607732
3507.022682	1064680.734617	43.612737
3507.007042	1064534.966808	43.617741
3506.966153	1064414.698072	43.622746
3507.227391	1064299.188127	43.627751
3507.005257	1064146.708366	43.632756
3507.197573	1064020.811471	43.637761
3507.109091	1063887.933093	43.642765
3507.235305	1063752.610313	43.647770
3507.175250	1063633.578664	43.652775
3507.038821	1063480.777597	43.657780
3506.831736	1063353.583866	43.662785
3507.035532	1063224.683397	43.667789
3507.207076	1063077.594941	43.672794
3506.932834	1062959.257676	43.677799
3507.377516	1062834.350760	43.682804
3507.185177	1062696.263208	43.687809
3506.833066	1062558.198499	43.692813
3507.398006	1062429.027391	43.697818
3506.972230	1062307.717106	43.702823
3507.308451	1062166.256397	43.707828
3507.188270	1062044.119876	43.712833
3506.917020	1061913.726704	43.717837
3506.767490	1061765.404575	43.722842
3506.795389	1061648.529614	43.727847
3506.794542	1061518.948975	43.732852
3507.076049	1061405.107787	43.737857
3507.030628	1061271.100032	43.742861
3507.180287	1061145.721986	43.747866
3506.964337	1061016.261212	43.752871
3507.039095	1060883.668443	43.757876
3506.856208	1060757.758625	43.762881
3507.043029	1060621.867380	43.767885
3507.015653	1060493.229832	43.772890
3506.366442	1060373.550594	43.777895
3506.770414	1060231.162348	43.782900
3506.246744	1060125.708655	43.787905
3506.611833	1060000.365331	43.792909
3506.527867	1059881.256378	43.797914
3506.257663	1059762.368125	43.802919
3506.444174	1059638.394216	43.807924
3506.540109	1059529.648978	43.812929
3506.458560	1059397.720303	43.817933
3506.887440	1059274.179827	43.822938
3506.699589	1059162.006850	43.827943
3506.641832	1059032.954923	43.832948
3506.541659	1058916.813561	43.837953
3506.231965	1058789.723782	43.842957
3506.272146	1058677.792343	43.847962
3506.604991	1058558.778775	43.852967
3506.258674	1058432.553701	43.857972
3506.448802	1058334.172575	43.862977
3506.285978	1058201.746993	43.867981
3506.635949	1058082.623992	43.872986
3506.173531	1057972.687651	43.877991
3506.190440	1057849.568423	43.882996
3506.280443	1057739.343768	43.888001
3506.134988	1057622.797222	43.893005
3506.482452	1057504.529206	43.898010
3506.204273	1057396.092490	43.903015
3506.089321	1057275.198068	43.908020
3506.434991	1057163.570941	43.913025
3506.250464	1057048.656611	43.918029
3506.246423	1056934.384626	43.923034
3506.204864	1056834.762314	43.928039
3506.499526	1056707.524951	43.933044
3506.542698	1056592.370894	43.938049
3506.007468	1056479.911425	43.943053
3506.623688	1056360.032835	43.948058
3506.288722	1056246.379268	43.953063
3506.421319	1056123.298792	43.958068
3506.700072	1056013.297641	43.963073
3506.231685	1055885.588778	43.968077
3506.466502	1055771.831585	43.973082
3506.016028	1055664.738395	43.978087
3506.015036	1055533.089398	43.983092
3506.206073	1055424.825746	43.988097
3505.911004	1055329.555036	43.993101
3506.299329	1055211.520264	43.998106
3506.132769	1055101.767048	44.003111
3506.647501	1054995.658509	44.008116
3506.184171	1054879.588246	44.013121
3505.906215	1054755.773769	44.018125
3506.116890	1054642.286439	44.023130
3506.123024	1054542.036496	44.028135
3506.293918	1054423.731509	44.033140
3506.265119	1054312.301160	44.038145
3506.058906	1054204.078988	44.043149
3506.372729	1054079.862678	44.048154
3505.789915	1053984.230510	44.053159
3505.956790	1053857.623301	44.058164
3505.884829	1053756.311481	44.063169
3505.915551	1053654.788070	44.068173
3506.157943	1053547.539646	44.073178
3506.007800	1053440.064550	44.078183
3505.838965	1053321.984735	44.083188
3505.877538	1053222.958896	44.088193
3505.921164	1053116.602597	44.093197
3505.912773	1053000.417864	44.098202
3505.438358	1052904.749126	44.103207
3505.729175	1052796.417491	44.108212
3506.060382	1052694.923370	44.113217
3506.031734	1052590.786660	44.118221
3506.111756	1052483.255032	44.123226
3506.054505	1052366.197133	44.128231
3505.922760	1052263.228415	44.133236
3505.933944	1052160.234237	44.138241
3506.048341	1052043.141223	44.143245
3505.996683	1051927.423236	44.148250
3505.898137	1051827.141239	44.153255
3505.815123	1051712.484773	44.158260
3505.903599	1051614.386317	44.163265
3505.699249	1051516.430794	44.168269
3505.607427	1051408.906561	44.173274
3505.444959	1051314.219819	44.178279
3505.585170	1051199.226587	44.183284
3505.691165	1051101.405499	44.188289
3505.192085	1051014.003123	44.193293
3505.472561	1050913.159835	44.198298
3505.044138	1050809.634139	44.203303
3505.560016	1050712.896184	44.208308
3505.451964	1050618.188555	44.213313
3505.457206	1050518.637420	44.218317
3505.508376	1050417.533469	44.223322
3505.452414	1050327.635595	44.228327
3505.568395	1050226.131599	44.233332
3505.683336	1050124.240027	44.238337
3505.620420	1050026.234796	44.243341
3505.252094	1049915.061063	44.248346
3505.424421	1049831.870780	44.253351
3505.247408	1049736.001678	44.258356
3505.492425	1049642.762842	44.263361
3505.429602	1049552.467578	44.268365
3505.804396	1049449.363002	44.273370
3505.318058	1049350.836639	44.278375
3505.291445	1049260.627132	44.283380
3505.550699	1049150.396014	44.288385
3505.120125	1049055.039311	44.293389
3505.708996	1048958.258669	44.298394
3505.311280	1048862.507268	44.303399
3505.646765	1048770.879232	44.308404
3505.276176	1048670.005792	44.313409
3505.151786	1048571.598925	44.318413
3505.185654	1048477.410248	44.323418
3505.306820	1048397.487832	44.328423
3505.120929	1048291.848501	44.333428
3505.455733	1048194.710350	44.338433
3505.191407	1048102.591014	44.343437
3505.338026	1047998.821458	44.348442
3505.161913	1047914.019091	44.353447
3505.145336	1047823.977530	44.358452
3505.562760	1047737.723548	44.363457
3505.179975	1047639.632205	44.368461
3505.174239	1047535.782550	44.373466
3505.363326	1047447.148737	44.378471
3505.298042	1047354.694614	44.383476
3505.206877	1047262.532775	44.388481
3504.990047	1047159.289953	44.393485
3505.313041	1047066.960124	44.398490
3505.067313	1046978.390424	44.403495
3505.263608	1046888.974283	44.408500
3504.927666	1046799.065182	44.413505
3505.186156	1046703.071797	44.418509
3504.967793	1046601.170256	44.423514
3505.275359	1046526.982112	44.428519
3505.207879	1046428.045092	44.433524
3505.104293	1046346.199372	44.438529
3504.897306	1046247.668255	44.443533
3505.074514	1046161.332763	44.448538
3504.778061	1046072.756930	44.453543
3504.663088	1045979.708784	44.458548
3504.928992	1045899.629941	44.463553
3504.729535	1045820.109318	44.468557
3504.895959	1045730.486312	44.473562
3504.921507	1045656.429514	44.478567
3504.686129	1045575.076854	44.483572
3504.835237	1045489.121722	44.488577
3504.647693	1045416.738205	44.493581
3504.841413	1045327.297292	44.498586
3504.401410	1045249.835755	44.503591
3504.802919	1045163.158106	44.508596
3505.027306	1045086.453882	44.513601
3504.740221	1044994.479690	44.518605
3504.785744	1044908.146369	44.523610
3504.623471	1044828.219136	44.528615
3504.502953	1044744.228138	44.533620
3504.979703	1044661.296297	44.538625
3504.974138	1044580.084311	44.543629
3505.102362	1044490.447553	44.548634
3504.899426	1044421.433505	44.553639
3504.800673	1044325.071497	44.558644
3505.031621	1044223.052210	44.563649
3504.837169	1044149.687538	44.568653
3504.915554	1044058.699954	44.573658
3505.083778	1043967.985818	44.578663
3504.793269	1043893.957531	44.583668
3504.981202	1043809.032345	44.588673
3504.631484	1043717.433600	44.593677
3505.078195	1043634.877705	44.598682
3504.696806	1043557.576020	44.603687
3504.956405	1043458.918468	44.608692
3505.017365	1043385.501618	44.613697
3504.563675	1043295.748218	44.618701
3504.769849	1043220.470051	44.623706
3504.766811	1043140.009295	44.628711
3504.840956	1043043.016977	44.633716
3504.904138	1042971.139795	44.638721
3504.808972	1042887.985869	44.643725
3504.866891	1042799.878935	44.648730
3504.611113	1042717.714899	44.653735
3504.428740	1042639.788037	44.658740
3504.509627	1042559.401642	44.663745
3504.520801	1042485.208255	44.668749
3504.594479	1042394.483968	44.673754
3504.535160	1042319.816951	44.678759
3504.595073	1042238.173463	44.683764
3504.561374	1042166.881475	44.688769
3504.475173	1042087.481866	44.693773
3504.718237	1042012.567691	44.698778
3504.678140	1041931.998912	44.703783
3504.694737	1041855.477477	44.708788
3504.885805	1041773.322476	44.713793
3504.466071	1041687.402124	44.718797
3504.754794	1041611.991935	44.723802
3504.628467	1041541.383509	44.728807
3504.618310	1041451.430588	44.733812
3504.688447	1041368.033417	44.738817
3504.537756	1041287.570124	44.743821
3504.676029	1041203.966017	44.748826
3504.519854	1041131.811269	44.753831
3504.462902	1041059.445981	44.758836
3504.374185	1040988.437810	44.763841
3504.130811	1040909.723656	44.768845
3504.503788	1040834.868836	44.773850
3504.570796	1040759.483594	44.778855
3504.486753	1040684.991930	44.783860
3504.280447	1040616.510900	44.788865
3504.075594	1040537.978405	44.793869
3504.322885	1040450.769387	44.798874
3504.160913	1040378.895728	44.803879
3504.180491	1040320.424515	44.808884
3504.521389	1040234.646322	44.813889
3504.173893	1040157.678240	44.818893
3504.465940	1040091.621430	44.823898
3503.962949	1040024.245068	44.828903
3504.212300	1039950.268524	44.833908
3504.385392	1039884.228842	44.838913
3504.055489	1039823.780317	44.843917
3504.152232	1039733.105405	44.848922
3504.511140	1039664.519547	44.853927
3503.953444	1039601.206508	44.858932
3504.102438	1039525.887682	44.863937
3504.232604	1039461.106571	44.868941
3504.314225	1039394.979486	44.873946
3504.214323	1039311.482791	44.878951
3504.005102	1039237.282309	44.883956
3504.421455	1039168.004242	44.888961
3504.044377	1039100.209277	44.893965
3504.354017	1039035.296984	44.898970
3504.266274	1038967.066083	44.903975
3503.989674	1038888.328750	44.908980
3504.326067	1038817.222810	44.913985
3503.945121	1038753.000971	44.918989
3503.944991	1038674.021728	44.923994
3503.837275	1038613.813450	44.928999
3503.909777	1038546.131022	44.934004
3504.310030	1038481.294014	44.939009
3503.884712	1038413.981990	44.944013
3504.027704	1038344.158637	44.949018
3504.076194	1038280.150634	44.954023
3503.879231	1038215.505568	44.959028
3503.800884	1038142.525738	44.964033
3503.559427	1038084.460715	44.969037
3503.816413	1038025.732899	44.974042
3503.869702	1037966.554597	44.979047
3503.722892	1037890.682245	44.984052
3503.788434	1037828.309868	44.989057
3503.912205	1037777.142833	44.994061
3504.194451	1037696.169468	44.999066
3504.129378	1037642.325038	45.004071
3504.008299	1037559.192267	45.009076
3503.973798	1037485.519763	45.014081
3504.070260	1037436.481306	45.019085
3504.385015	1037368.067800	45.024090
3503.972980	1037300.256629	45.029095
3503.788962	1037229.409503	45.034100
3504.044746	1037159.746103	45.039105
3503.752749	1037103.032912	45.044109
3504.325029	1037033.315803	45.049114
3503.828545	1036954.780693	45.054119
3503.835639	1036899.853482	45.059124
3503.802376	1036837.389570	45.064129
3503.885269	1036780.127828	45.069133
3504.013350	1036696.264198	45.074138
3504.105298	1036646.542589	45.079143
3504.336325	1036572.524147	45.084148
3503.896327	1036492.135759	45.089153
3503.794231	1036442.057447	45.094157
3503.807969	1036383.932633	45.099162
3503.645725	1036313.457098	45.104167
3503.779612	1036244.672732	45.109172
3504.008516	1036183.028714	45.114177
3503.632633	1036144.501780	45.119181
3503.800294	1036074.259025	45.124186
3504.045402	1036002.455154	45.129191
3504.156870	1035939.183587	45.134196
3503.900924	1035867.750657	45.139201
3503.528298	1035810.553966	45.144205
3503.834869	1035736.221805	45.149210
3503.713439	1035688.944833	45.154215
3503.437631	1035639.758415	45.159220
3503.712552	1035563.011068	45.164225
3503.626727	1035513.792247	45.169229
3503.710324	1035450.229537	45.174234
3503.831959	1035400.008274	45.179239
3503.357738	1035333.537545	45.184244
3503.867601	1035273.675039	45.189249
3503.428538	1035205.939507	45.194253
3503.554905	1035153.780622	45.199258
3503.780232	1035103.442876	45.204263
3503.491790	1035044.289784	45.209268
3503.652220	1034984.675195	45.214273
3503.431274	1034926.283612	45.219277
3503.552920	1034870.156676	45.224282
3503.449631	1034822.869361	45.229287
3503.062474	1034762.181725	45.234292
3503.527751	1034699.224755	45.239297
3503.352781	1034639.855196	45.244301
3503.540999	1034594.065781	45.249306
3503.419996	1034543.199565	45.254311
3503.096969	1034483.465753	45.259316
3503.537263	1034428.926535	45.264321
3502.888118	1034390.045470	45.269325
3503.258416	1034328.067406	45.274330
3503.437063	1034281.406282	45.279335
3503.431674	1034231.001909	45.284340
3503.396595	1034163.767642	45.289345
3503.530721	1034130.270456	45.294349
3503.339329	1034082.701117	45.299354
3503.344014	1034021.940874	45.304359
3503.562118	1033972.077859	45.309364
3503.626417	1033900.470186	45.314369
3503.422108	1033847.289245	45.319373
3503.624301	1033780.978828	45.324378
3503.228648	1033739.052029	45.329383
3503.307557	1033682.920176	45.334388
3503.806853	1033625.654178	45.339393
3503.419993	1033572.694198	45.344397
3503.386337	1033523.255673	45.349402
3503.249433	1033468.028043	45.354407
3503.033038	1033414.844963	45.359412
3503.499027	1033376.644007	45.364417
3503.115034	1033325.229406	45.369421
3503.337137	1033263.747742	45.374426
3503.231801	1033215.963298	45.379431
3503.288872	1033162.829538	45.384436
3503.650352	1033110.612812	45.389441
3503.435591	1033058.877576	45.394445
3503.447929	1033000.911223	45.399450
3503.426143	1032943.627280	45.404455
3503.203021	1032893.440210	45.409460
3503.538193	1032846.741304	45.414465
3503.216746	1032785.924528	45.419469
3503.733798	1032729.227048	45.424474
3503.602251	1032685.506881	45.429479
3503.241812	1032636.017533	45.434484
3503.206176	1032565.376926	45.439489
3503.271369	1032524.139289	45.444493
3503.304949	1032468.002671	45.449498
3503.340538	1032430.737140	45.454503
3503.311252	1032388.739829	45.459508
3503.250872	1032319.939007	45.464513
3503.240865	1032268.356271	45.469517
3503.222990	1032225.097682	45.474522
3503.459238	1032175.215617	45.479527
3503.222682	1032116.603578	45.484532
3503.618700	1032072.888502	45.489537
3503.344726	1032025.508768	45.494541
3503.495165	1031966.637842	45.499546
3503.287380	1031919.052727	45.504551
3503.094223	1031875.142775	45.509556
3503.598787	1031814.469720	45.514561
3503.334434	1031768.538065	45.519565
3503.191452	1031715.326673	45.524570
3503.519175	1031656.036106	45.529575
3503.222661	1031615.335288	45.534580
3503.636815	1031562.127468	45.539585
3503.433204	1031500.696492	45.544589
3503.198699	1031451.079080	45.549594
3503.500437	1031402.050487	45.554599
3503.147448	1031346.837428	45.559604
3503.310737	1031292.700378	45.564609
3503.565091	1031251.034981	45.569613
3503.664260	1031194.293946	45.574618
3503.742366	1031142.976694	45.579623
3503.451689	1031088.525227	45.584628
3503.940342	1031022.522051	45.589633
3503.461281	1030960.452865	45.594637
3503.530661	1030915.814485	45.599642
3503.656316	1030860.808197	45.604647
3503.077474	1030803.400403	45.609652
3503.243605	1030750.516125	45.614657
3502.831443	1030704.503238	45.619661
3503.143720	1030650.625852	45.624666
3503.675144	1030609.103654	45.629671
3503.428108	1030560.158054	45.634676
3503.566375	1030493.238217	45.639681
3503.257731	1030454.563989	45.644685
3503.537221	1030391.492213	45.649690
3503.279191	1030339.254787	45.654695
3502.917404	1030279.385458	45.659700
3503.419365	1030238.349443	45.664705
3503.317117	1030200.607633	45.669709
3503.442940	1030151.887494	45.674714
3503.414964	1030100.384492	45.679719
3503.299917	1030038.535546	45.684724
3503.542168	1029992.312179	45.689729
3502.676658	1029951.596102	45.694733
3503.382155	1029890.965890	45.699738
3503.415441	1029848.358208	45.704743
3503.198438	1029791.848640	45.709748
3503.750125	1029731.726160	45.714753
3503.443186	1029690.141567	45.719757
3503.083100	1029631.620579	45.724762
3503.294270	1029578.524130	45.729767
3503.081037	1029525.787565	45.734772
3503.404775	1029480.708500	45.739777
3503.132667	1029437.373338	45.744781
3503.199959	1029375.293350	45.749786
3503.466896	1029329.931928	45.754791
3502.968702	1029285.083490	45.759796
3503.313481	1029246.390098	45.764801
3503.143460	1029212.235639	45.769805
3502.809312	1029144.505931	45.774810
3503.133444	1029085.091831	45.779815
3502.975663	1028976.465562	45.784820
3503.110934	1028799.612413	45.789825
3502.727828	1028587.587250	45.794829
3502.988987	1028298.161439	45.799834
3502.798288	1027952.908916	45.804839
3502.766928	1027539.901258	45.809844
3502.951746	1027072.773084	45.814849
3502.561270	1026531.780528	45.819853
3502.553050	1025905.795603	45.824858
3502.478779	1025238.276778	45.829863
3502.420156	1024521.539373	45.834868
3501.987485	1023712.204078	45.839873
3501.796941	1022849.004468	45.844877
3501.814007	1021910.977764	45.849882
3502.084156	1020904.770550	45.854887
3501.777430	1019821.559161	45.859892
3501.378961	1018650.062110	45.864897
3501.040238	1017421.737117	45.869901
3501.019764	1016120.683495	45.874906
3500.770073	1014721.504746	45.879911
3500.594025	1013263.408041	45.884916
3500.501561	1011723.810423	45.889921
3500.080350	1010109.029085	45.894925
3499.566426	1008397.966858	45.899930
3499.648478	1006619.493661	45.904935
3499.083482	1004760.524178	45.909940
3499.254978	1002809.271294	45.914945
3498.650763	1000792.946045	45.919949
3497.981952	998688.774563	45.924954
3497.961741	996498.587836	45.929959
3497.597969	994232.486996	45.934964
3497.257090	991889.542095	45.939969
3496.425047	989456.286313	45.944973
3496.636327	986945.523495	45.949978
3496.126703	984346.901967	45.954983
3495.538486	981671.525323	45.959988
3495.026352	978909.687505	45.964993
3494.590010	976059.212720	45.969997
3494.733978	973143.066373	45.975002
3494.119523	970142.682081	45.980007
3493.341003	967054.797471	45.985012
3492.846544	963871.070275	45.990017
3492.450939	960639.303572	45.995021
3492.014870	957297.561896	46.000026
3491.216601	953895.855297	46.005031
3490.545690	950499.712664	46.010036
3490.407528	947010.831621	46.015041
3489.628962	943439.200289	46.020045
3488.918786	939787.233936	46.025050
3488.210314	936074.562948	46.030055
3487.336267	932264.325957	46.035060
3487.027639	928376.875824	46.040065
3485.945836	924419.308156	46.045069
3485.603952	920382.965605	46.050074
3484.869358	916254.207122	46.055079
3483.827587	912046.330863	46.060084
3483.276904	907767.252047	46.065089
3481.956193	903414.726795	46.070093
3481.344048	898968.757758	46.075098
3480.804590	894457.207151	46.080103
3479.630725	889866.522044	46.085108
3479.106784	885167.572505	46.090113
3478.038723	880424.013551	46.095117
3477.002301	875586.886064	46.100122
3476.216798	870668.781381	46.105127
3475.217499	865678.267395	46.110132
3474.269233	860601.745135	46.115137
3473.020645	855431.317971	46.120141
3471.952208	850193.995344	46.125146
3471.574782	844879.825729	46.130151
3470.349634	839481.846608	46.135156
3469.278034	833998.123041	46.140161
3468.387617	828444.616792	46.145165
3467.036355	822801.308252	46.150170
3466.074582	817075.868049	46.155175
3465.021304	811268.669042	46.160180
3463.977965	805386.464698	46.165185
3462.854754	799418.297304	46.170189
3461.999549	793369.362202	46.175194
3460.828131	787234.457704	46.180199
3459.154172	781021.489415	46.185204
3458.317461	774712.480557	46.190209
3456.883836	768330.226170	46.195213
3455.661995	761879.865656	46.200218
3454.529553	755341.973326	46.205223
3453.196539	748727.284886	46.210228
3452.157179	742018.103612	46.215233
3450.679486	735245.147389	46.220237
3449.096554	728374.504531	46.225242
3448.088787	721427.735705	46.230247
3446.450497	714393.585771	46.235252
3444.747076	707277.461825	46.240257
3443.191326	700101.207558	46.245261
3441.792694	692828.613314	46.250266
3440.672028	685490.809163	46.255271
3439.153852	678069.725779	46.260276
3437.984225	670571.194967	46.265281
3436.191981	662988.926698	46.270285
3434.615155	655326.508091	46.275290
3432.688482	647593.323464	46.280295
3431.011496	639778.687058	46.285300
3429.982391	631882.984228	46.290305
3427.794741	623937.334199	46.295309
3425.820601	615892.904049	46.300314
3424.705619	607769.487344	46.305319
3422.294417	599584.892390	46.310324
3420.679699	591335.278600	46.315329
3419.021860	583011.652056	46.320333
3417.031570	574602.896196	46.325338
3415.640833	566131.605968	46.330343
3413.363015	557580.584938	46.335348
3411.560288	548937.875881	46.340353
3409.021040	540264.918881	46.345357
3407.360005	531503.064094	46.350362
3405.478245	522669.733229	46.355367
3403.053030	513771.605053	46.360372
3401.197493	504805.485842	46.365377
3399.250811	495780.817957	46.370381
3397.147629	486690.268431	46.375386
3394.725387	477507.064894	46.380391
3392.603283	468286.644769	46.385396
3390.486566	458998.536345	46.390401
3388.094819	449634.021221	46.395405
3385.873560	440221.848197	46.400410
3383.803616	430729.382755	46.405415
3381.134693	421194.059007	46.410420
3378.713635	411583.245231	46.415425
3375.946320	401915.394688	46.420429
3373.504051	392187.539072	46.425434
3371.092607	382419.116760	46.430439
3368.121895	372603.070884	46.435444
3365.705310	362724.303571	46.440449
3362.766082	352802.517758	46.445453
3359.838911	342823.687397	46.450458
3357.456065	332801.779027	46.455463
3354.110277	322744.137332	46.460468
3351.433667	312616.940332	46.465473
3348.378883	302473.599307	46.470477
3344.838480	292293.118606	46.475482
3342.065851	282055.624644	46.480487
3338.478178	271809.763505	46.485492
3335.139610	261502.825991	46.490497
3331.769268	251184.836660	46.495501
3328.714093	240831.431368	46.500506
3325.216868	230443.901292	46.505511
3321.802424	219962.398210	46.510516
3318.160357	209520.908376	46.515521
3314.206551	199080.901888	46.520525
3310.380229	188615.796233	46.525530
3306.428596	178133.065208	46.530535
3301.941531	167660.012675	46.535540
3298.115147	157164.313746	46.540545
3293.516762	146688.056344	46.545549
3288.944451	136209.465091	46.550554
3284.137174	125732.186829	46.555559
3279.038093	115285.398628	46.560564
3273.679874	104860.884688	46.565569
3268.155443	94463.170948	46.570573
3262.005471	84100.136863	46.575578
3255.696673	73784.963104	46.580583
3248.995748	63562.004223	46.585588
3241.533671	53393.685253	46.590593
3233.328885	43335.480521	46.595597
3221.984587	33448.141495	46.600602
3202.336966	23922.965572	46.605607
3158.525483	15306.255325	46.610612
3100.435321	7606.544714	46.615617
3016.464070	1435.544598	46.620621
2793.642013	388.020565	46.625626
2631.056072	370.808330	46.630631
2586.435709	376.713633	46.635636
2631.332749	380.425757	46.640641
2716.930163	363.924684	46.645645
2799.152367	355.525008	46.650650
2857.028321	328.071069	46.655655
2883.691681	329.386116	46.660660
2885.994396	326.681341	46.665665
2875.944217	341.045267	46.670669
2861.937508	339.898016	46.675674
2850.395251	337.016765	46.680679
2842.993832	322.307141	46.685684
2838.785322	316.853939	46.690689
2837.446214	317.366446	46.695693
2836.125578	329.051054	46.700698
2835.230364	328.501529	46.705703
2833.169616	330.290762	46.710708
2830.858731	313.008027	46.715713
2828.354393	308.862191	46.720717
2825.141057	314.021692	46.725722
2821.834099	309.740319	46.730727
2818.594911	311.354946	46.735732
2815.942276	307.040094	46.740737
2812.860092	312.260257	46.745741
2809.729938	304.973812	46.750746
2806.389040	300.060810	46.755751
2802.756472	310.859287	46.760756
2799.675425	296.323824	46.765761
2797.212282	300.694202	46.770765
2793.448404	299.435295	46.775770
2790.470583	289.003389	46.780775
2787.282976	303.875114	46.785780
2783.710780	297.144001	46.790785
2781.015059	296.159770	46.795789
2777.323132	296.781867	46.800794
2774.027629	282.397711	46.805799
2770.384239	294.928239	46.810804
2767.365262	296.410093	46.815809
2764.317007	293.127241	46.820813
2760.512578	298.106389	46.825818
2757.406339	297.439650	46.830823
2754.055507	296.128549	46.835828
2750.452835	288.613019	46.840833
2747.132966	278.399531	46.845837
2744.006268	302.079189	46.850842
2740.993605	294.133908	46.855847
2737.148829	288.374953	46.860852
2733.833426	291.550519	46.865857
2730.376683	282.987760	46.870861
2726.764906	285.395992	46.875866
2723.732170	287.983818	46.880871
2720.067876	285.253126	46.885876
2716.403583	286.684230	46.890881
2713.186094	288.951100	46.895885
2709.924389	281.353728	46.900890
2706.936051	274.048702	46.905895
2703.256619	274.613228	46.910900
2699.557716	271.673773	46.915905
2696.016082	268.177906	46.920909
2692.960983	272.275048	46.925914
2689.262468	269.210633	46.930919
2685.755209	267.480113	46.935924
2682.474596	256.779344	46.940929
2679.632715	261.925781	46.945933
2675.835248	260.518766	46.950938
2672.439524	257.488298	46.955943
2668.523600	266.674283	46.960948
2665.039181	260.772598	46.965953
2661.421776	268.215017	46.970957
2658.183503	267.669142	46.975962
2655.800030	266.530181	46.980967
2651.670790	259.473973	46.985972
2647.831721	259.629864	46.990977
2644.361048	257.162574	46.995981
2640.673599	253.844983	47.000986
2637.977822	256.315320	47.005991
2634.289180	257.100615	47.010996
2630.667142	247.778683	47.016001
2627.625494	253.192286	47.021005
2624.010571	253.563400	47.026010
2620.958883	257.961894	47.031015
2616.832636	254.003370	47.036020
2613.234026	263.064048	47.041025
2609.829518	256.207824	47.046029
2606.436935	252.952128	47.051034
2603.619107	254.511962	47.056039
2599.546951	248.980015	47.061044
2596.052627	244.093320	47.066049
2593.041720	249.348254	47.071053
2588.965127	246.664210	47.076058
2585.412544	248.909425	47.081063
2581.898373	246.586277	47.086068
2578.762831	253.828707	47.091073
2575.665056	254.695764	47.096077
2571.642104	250.941721	47.101082
2568.403820	247.526625	47.106087
2565.159073	260.962649	47.111092
2561.563064	250.605193	47.116097
2558.407546	255.045099	47.121101
2554.253890	261.415271	47.126106
2551.346713	243.900077	47.131111
2547.331258	258.434474	47.136116
2543.847931	250.986018	47.141121
2540.609061	248.119272	47.146125
2536.577005	253.605551	47.151130
2533.717963	242.951872	47.156135
2530.045774	249.753903	47.161140
2526.570106	253.640656	47.166145
2523.252080	246.531568	47.171149
2519.801076	249.479672	47.176154
2515.991817	247.727507	47.181159
2512.573778	241.060529	47.186164
2509.044676	248.640270	47.191169
2505.643285	241.666290	47.196173
2502.207708	241.830500	47.201178
2499.128820	246.044294	47.206183
2495.169363	238.362429	47.211188
2491.856507	243.300969	47.216193
2488.449865	238.833078	47.221197
2484.848848	244.342715	47.226202
2481.321380	243.416333	47.231207
2477.807460	239.488825	47.236212
2474.178539	240.000339	47.241217
2470.786292	231.467268	47.246221
2467.400456	237.630648	47.251226
2464.000292	230.981962	47.256231
2460.487707	237.272007	47.261236
2456.559577	231.897831	47.266241
2453.436897	223.828604	47.271245
2449.987716	234.362996	47.276250
2446.785407	227.155455	47.281255
2443.196207	234.842501	47.286260
2439.480339	235.178454	47.291265
2435.886890	226.576375	47.296269
2432.046291	233.768877	47.301274
2429.110829	229.860742	47.306279
2425.380745	227.357021	47.311284
2421.956862	238.340091	47.316289
2418.729259	216.205034	47.321293
2414.904180	219.209340	47.326298
2412.049968	229.383197	47.331303
2408.107473	228.090609	47.336308
2404.441203	223.278152	47.341313
2400.825463	220.045552	47.346317
2397.318004	220.663254	47.351322
2393.815453	222.856398	47.356327
2390.429984	226.573533	47.361332
2387.111293	231.536947	47.366337
2384.103341	226.139123	47.371341
2380.079912	232.172187	47.376346
2376.607145	223.992522	47.381351
2373.099908	222.766983	47.386356
2369.826871	224.640423	47.391361
2366.543914	230.854452	47.396365
2362.314891	223.042607	47.401370
2359.332895	219.099165	47.406375
2355.675528	219.809880	47.411380
2352.150648	227.597143	47.416385
2348.621967	221.477605	47.421389
2345.105320	227.600348	47.426394
2341.976211	218.210132	47.431399
2338.352170	222.075649	47.436404
2334.842490	226.032409	47.441409
2331.226071	218.150632	47.446413
2327.502082	231.450466	47.451418
2324.220114	222.457405	47.456423
2320.216640	220.839685	47.461428
2317.099889	223.156980	47.466433
2314.037225	222.004064	47.471437
2310.129402	218.817314	47.476442
2306.645215	214.990361	47.481447
2303.184063	220.174812	47.486452
2299.680335	223.716343	47.491457
2296.478594	211.654360	47.496461
2292.681958	227.220106	47.501466
2289.498142	212.149676	47.506471
2285.883390	214.481042	47.511476
2282.213541	227.111350	47.516481
2278.873924	220.986714	47.521485
2275.260776	226.863860	47.526490
2271.747968	216.933675	47.531495
2268.328475	219.401550	47.536500
2264.642615	221.099733	47.541505
2261.499434	210.200259	47.546509
2257.665627	223.884834	47.551514
2254.101172	210.928683	47.556519
2250.787397	214.339655	47.561524
2246.997662	225.214115	47.566529
2243.870264	211.737685	47.571533
2240.401464	218.922413	47.576538
2237.189540	214.347856	47.581543
2233.514651	213.624282	47.586548
2229.683059	216.637840	47.591553
2226.367686	218.182592	47.596557
2222.800973	221.935311	47.601562
2219.281015	214.288772	47.606567
2215.721695	220.319255	47.611572
2212.212207	209.798494	47.616577
2209.127678	207.935742	47.621581
2205.472999	222.104890	47.626586
2202.085591	207.815917	47.631591
2198.197316	209.861147	47.636596
2194.665681	210.164860	47.641601
2191.350109	211.653917	47.646605
2187.530714	216.914077	47.651610
2183.819220	200.849966	47.656615
2180.658264	215.780707	47.661620
2177.361963	214.344369	47.666625
2174.146171	200.271783	47.671629
2170.701423	209.300609	47.676634
2167.070168	207.157991	47.681639
2163.385489	214.770517	47.686644
2159.499097	208.866361	47.691649
2156.400692	208.139391	47.696653
2152.485685	215.140848	47.701658
2149.442716	207.955822	47.706663
2146.071500	215.339660	47.711668
2142.076786	209.759317	47.716673
2139.056870	210.141730	47.721677
2135.419473	206.018024	47.726682
2131.952527	208.571821	47.731687
2128.407833	208.950134	47.736692
2124.520342	202.575786	47.741697
2121.441251	202.186308	47.746701
2117.597556	214.465906	47.751706
2114.229191	216.375992	47.756711
2110.708149	207.356588	47.761716
2107.181651	225.311802	47.766721
2104.356884	207.308774	47.771725
2100.424900	209.362546	47.776730
2097.248827	211.990516	47.781735
2093.645916	206.478465	47.786740
2089.689551	212.484615	47.791745
2086.211343	212.477182	47.796749
2082.551458	207.947589	47.801754
2079.456745	210.797443	47.806759
2075.708963	206.016669	47.811764
2072.506155	213.024890	47.816769
2068.843499	199.188370	47.821773
2065.041665	213.457108	47.826778
2061.758288	203.493747	47.831783
2058.465355	201.951741	47.836788
2054.803887	210.108421	47.841793
2051.359362	199.721972	47.846797
2047.994725	213.161406	47.851802
2044.326612	205.251035	47.856807
2040.983159	205.063248	47.861812
2037.383872	211.276694	47.866817
2034.098742	199.169529	47.871821
2029.919765	199.996142	47.876826
2026.875181	202.048886	47.881831
2023.473936	209.799989	47.886836
2019.819593	209.738476	47.891841
2016.086826	195.225428	47.896845
2012.789939	201.868764	47.901850
2009.546611	206.531118	47.906855
2005.823664	200.012395	47.911860
2001.956588	203.168062	47.916865
1998.937237	196.993609	47.921869
1995.474771	202.746759	47.926874
1991.920056	213.788537	47.931879
1988.795753	195.351486	47.936884
1984.830847	194.585907	47.941889
1981.716145	200.348187	47.946893
1977.614605	204.595312	47.951898
1974.274571	197.162229	47.956903
1970.849337	196.391783	47.961908
1967.170527	199.883806	47.966913
1964.295097	207.022346	47.971917
1960.449993	199.092884	47.976922
1956.375015	189.228414	47.981927
1952.997741	192.198033	47.986932
1949.301070	199.522471	47.991937
1946.244984	189.639581	47.996941
1942.820066	192.770870	48.001946
1939.577022	193.032620	48.006951
1936.278770	191.472016	48.011956
1932.304834	198.328101	48.016961
1928.785206	196.025522	48.021965
1925.085159	201.960355	48.026970
1921.882536	190.304719	48.031975
1918.371639	197.258550	48.036980
1914.705391	196.425980	48.041985
1911.637736	186.995978	48.046989
1907.770859	199.166115	48.051994
1904.340480	199.446256	48.056999
1900.950600	196.605817	48.062004
1897.196635	194.405548	48.067009
1894.179004	195.483213	48.072013
1890.312480	195.387613	48.077018
1886.669945	193.466613	48.082023
1883.478612	190.764596	48.087028
1879.629813	203.927112	48.092033
1876.270771	193.773505	48.097037
1872.440863	194.154107	48.102042
1869.501863	191.664606	48.107047
1866.089659	194.548769	48.112052
1862.427155	191.813804	48.117057
1859.151655	179.334319	48.122061
1855.292275	188.772517	48.127066
1851.587395	195.954113	48.132071
1848.225643	187.629082	48.137076
1844.375955	190.786889	48.142081
1841.394014	184.315702	48.147085
1837.695345	196.565549	48.152090
1834.443317	196.184008	48.157095
1831.220246	182.571201	48.162100
1827.241641	185.942863	48.167105
1824.051958	192.232062	48.172109
1820.038640	192.392266	48.177114
1816.609023	190.551898	48.182119
1813.420353	187.224585	48.187124
1809.345794	194.965605	48.192129
1806.252761	193.101969	48.197133
1803.054534	197.297518	48.202138
1799.218705	191.262808	48.207143
1795.959360	193.849094	48.212148
1792.252031	188.087383	48.217153
1788.771672	199.461269	48.222157
1785.268877	193.685149	48.227162
1781.692496	184.701717	48.232167
1778.083527	185.757820	48.237172
1774.584594	187.026527	48.242177
1771.297842	171.472354	48.247181
1767.774190	187.435775	48.252186
1764.276765	186.514952	48.257191
1761.004169	181.185173	48.262196
1757.082493	183.818308	48.267201
1753.854424	174.758387	48.272205
1750.490531	189.673179	48.277210
1746.817616	190.407179	48.282215
1743.275922	185.564183	48.287220
1739.443364	182.547762	48.292225
1736.307204	183.104609	48.297229
1732.782120	186.474001	48.302234
1729.129604	186.488595	48.307239
1725.597486	189.753688	48.312244
1722.123254	187.832925	48.317249
1718.884448	183.210383	48.322253
1714.941445	182.982669	48.327258
1711.803170	188.654421	48.332263
1708.188492	178.772874	48.337268
1704.501815	187.511876	48.342273
1701.461453	183.616549	48.347277
1697.791571	182.061936	48.352282
1694.146630	189.377450	48.357287
1691.156592	181.945872	48.362292
1687.131513	186.069736	48.367297
1684.081505	176.672367	48.372301
1679.957948	182.233036	48.377306
1676.309687	183.174325	48.382311
1672.793963	172.855311	48.387316
1669.630893	184.330581	48.392321
1666.346746	183.444265	48.397325
1662.386430	177.590009	48.402330
1659.308781	181.527558	48.407335
1655.563421	179.219060	48.412340
1652.166631	177.999037	48.417345
1648.783441	176.655918	48.422349
1645.213285	177.425793	48.427354
1641.675385	184.647009	48.432359
1638.241160	171.006622	48.437364
1634.811413	180.212911	48.442369
1631.402956	174.730209	48.447373
1627.638667	180.484180	48.452378
1623.845190	184.766381	48.457383
1620.687042	169.638095	48.462388
1617.179838	175.567873	48.467393
1613.725090	173.649871	48.472397
1610.389544	178.096246	48.477402
1606.663798	180.407570	48.482407
1602.759685	177.795885	48.487412
1599.214414	177.803109	48.492417
1596.175896	178.861849	48.497421
1592.512459	172.884062	48.502426
1589.115585	174.504693	48.507431
1585.661715	163.752099	48.512436
1582.091058	179.772460	48.517441
1578.730264	178.590830	48.522445
1575.276351	173.464114	48.527450
1571.642801	181.264370	48.532455
1568.113274	176.057694	48.537460
1564.712940	185.787068	48.542465
1561.359500	173.483014	48.547469
1557.795894	174.074270	48.552474
1553.784433	184.296263	48.557479
1550.724590	166.926903	48.562484
1546.828369	180.911172	48.567489
1543.516162	181.320165	48.572493
1540.055919	172.600567	48.577498
1536.458305	173.713418	48.582503
1533.124385	175.731432	48.587508
1529.569861	180.536091	48.592513
1526.246141	168.904235	48.597517
1522.580386	177.440669	48.602522
1518.972209	185.220879	48.607527
1515.746126	175.582636	48.612532
1512.111984	184.079332	48.617537
1508.973932	177.447909	48.622541
1505.122739	173.788699	48.627546
1501.192499	173.096006	48.632551
1498.197553	164.657769	48.637556
1494.402472	175.588038	48.642561
1491.175768	164.891733	48.647565
1487.542876	181.428701	48.652570
1483.788454	178.218893	48.657575
1480.853130	182.479011	48.662580
1476.673505	180.845662	48.667585
1473.607172	171.816130	48.672589
1470.240501	177.269948	48.677594
1466.563337	176.543103	48.682599
1463.416970	177.938455	48.687604
1459.163737	182.547201	48.692609
1456.183146	166.673767	48.697613
1452.694884	178.441323	48.702618
1449.030332	172.081907	48.707623
1445.562244	167.519449	48.712628
1441.797355	170.217931	48.717633
1438.468667	166.172021	48.722637
1434.847453	163.747166	48.727642
1431.637905	173.723404	48.732647
1428.061645	167.796145	48.737652
1424.439880	167.326354	48.742657
1421.332402	161.042436	48.747661
1417.576861	162.530259	48.752666
1413.906915	171.707410	48.757671
1410.444679	160.584865	48.762676
1406.934300	169.476415	48.767681
1403.549771	159.816844	48.772685
1399.689747	168.656201	48.777690
1396.147443	167.885826	48.782695
1393.313758	164.752199	48.787700
1389.473863	173.201707	48.792705
1386.051175	161.857283	48.797709
1382.171274	168.620854	48.802714
1378.436139	168.262536	48.807719
1375.427490	160.093589	48.812724
1372.018957	167.351767	48.817729
1369.059053	162.441374	48.822733
1364.944504	165.707756	48.827738
1361.345494	164.420331	48.832743
1358.146368	175.884975	48.837748
1354.339999	170.602274	48.842753
1351.232826	158.027056	48.847757
1347.441678	163.901902	48.852762
1343.485164	167.833296	48.857767
1340.127008	165.013662	48.862772
1336.743851	171.083796	48.867777
1333.991030	161.603831	48.872781
1330.204635	162.074619	48.877786
1326.437742	171.303621	48.882791
1322.935361	166.474207	48.887796
1319.084977	169.877750	48.892801
1315.947725	156.229703	48.897805
1312.356231	166.623789	48.902810
1309.082361	160.583253	48.907815
1305.651079	167.956497	48.912820
1301.899280	174.221766	48.917825
1298.246881	165.075282	48.922829
1294.710080	164.095395	48.927834
1291.385971	166.116831	48.932839
1287.850406	170.112647	48.937844
1284.332644	160.690505	48.942849
1281.129561	159.515449	48.947853
1277.318313	151.362725	48.952858
1273.721290	166.345428	48.957863
1270.125284	162.823199	48.962868
1266.658243	167.755500	48.967873
1263.270386	156.701078	48.972877
1259.817982	151.092558	48.977882
1256.756579	162.921520	48.982887
1252.655624	170.286152	48.987892
1249.227429	164.703135	48.992897
1246.127815	164.485044	48.997901
1242.445325	153.530079	49.002906
1238.690455	163.542530	49.007911
1235.419886	159.080673	49.012916
1231.800754	168.568072	49.017921
1228.343191	154.703327	49.022925
1224.939541	158.770625	49.027930
1221.251835	162.013390	49.032935
1217.800296	153.258224	49.037940
1214.466576	164.064599	49.042945
1210.462423	161.472721	49.047949
1207.174621	156.046700	49.052954
1203.530590	157.830940	49.057959
1200.690639	154.853916	49.062964
1197.015145	160.957072	49.067969
1193.908790	164.829989	49.072973
1189.898988	163.603661	49.077978
1186.163350	169.642959	49.082983
1182.843379	163.564029	49.087988
1179.345596	157.897831	49.092993
1175.504895	158.367605	49.097997
1172.184582	159.142251	49.103002
1168.671762	163.778885	49.108007
1165.130499	155.352385	49.113012
1161.554288	156.119656	49.118017
1158.027503	145.046312	49.123021
1154.806370	154.833848	49.128026
1151.252373	153.561896	49.133031
1147.925681	148.105927	49.138036
1144.367169	159.193508	49.143041
1140.684823	150.225513	49.148045
1137.595862	155.377412	49.153050
1133.693388	155.757370	49.158055
1130.119425	152.863473	49.163060
1126.548027	163.490891	49.168065
1122.925732	156.712320	49.173069
1119.793083	155.778963	49.178074
1116.104153	155.622705	49.183079
1112.904596	141.100633	49.188084
1109.024361	153.742578	49.193089
1105.770460	156.901649	49.198093
1102.291530	153.759744	49.203098
1098.727700	161.164030	49.208103
1095.442683	152.778535	49.213108
1091.548412	147.434157	49.218113
1088.405560	158.689615	49.223117
1084.701988	154.668690	49.228122
1081.113044	145.787918	49.233127
1077.961542	150.960128	49.238132
1073.928734	152.728905	49.243137
1070.729163	145.812904	49.248141
1067.374221	148.910536	49.253146
1063.613253	152.152155	49.258151
1059.849490	149.372602	49.263156
1056.358960	155.349885	49.268161
1053.030918	145.205688	49.273165
1049.761776	150.239384	49.278170
1046.326492	157.346234	49.283175
1042.706052	152.476885	49.288180
1038.950694	162.082352	49.293185
1035.554520	145.072533	49.298189
1031.931538	150.177579	49.303194
1028.661129	162.704085	49.308199
1025.476745	136.342191	49.313204
1021.569380	164.171631	49.318209
1018.272077	145.193402	49.323213
1014.966808	150.038726	49.328218
1011.359631	150.648603	49.333223
1007.678847	143.557655	49.338228
1004.013498	157.342313	49.343233
1000.462771	155.665512	49.348237
997.113224	149.616829	49.353242
993.129947	145.047447	49.358247
990.268250	146.879220	49.363252
986.857622	156.960925	49.368257
982.964632	155.042408	49.373261
979.972639	149.668992	49.378266
976.097353	153.798784	49.383271
972.383554	148.471347	49.388276
969.320120	148.461393	49.393281
965.668308	146.629741	49.398285
961.943624	152.256138	49.403290
958.047799	158.033029	49.408295
955.164659	149.396383	49.413300
951.134770	155.777677	49.418305
948.435102	143.132466	49.423309
944.974214	148.181193	49.428314
940.991525	158.319784	49.433319
937.428033	159.805057	49.438324
933.610674	157.634350	49.443329
930.286925	156.530491	49.448333
927.363985	158.240500	49.453338
923.567057	158.477365	49.458343
920.366058	153.567442	49.463348
916.301697	154.139700	49.468353
913.263874	148.298860	49.473357
909.670046	146.841730	49.478362
906.015986	151.966077	49.483367
902.761934	149.319397	49.488372
898.722544	153.896105	49.493377
895.195084	144.509160	49.498381
891.816757	148.192505	49.503386
888.281171	152.774031	49.508391
885.263180	150.561433	49.513396
881.746072	149.843403	49.518401
878.171604	136.737632	49.523405
874.959345	144.105563	49.528410
870.796728	164.714295	49.533415
867.226122	139.904604	49.538420
863.874353	149.717664	49.543425
860.581225	151.608003	49.548429
857.116715	149.957888	49.553434
853.525124	150.134151	49.558439
850.177538	135.281043	49.563444
846.462256	147.290018	49.568449
842.778245	149.956216	49.573453
839.613706	152.195585	49.578458
835.867644	157.349071	49.583463
832.071203	140.461036	49.588468
828.735402	141.869699	49.593473
825.705920	148.084379	49.598477
822.179821	131.938396	49.603482
818.347142	156.586053	49.608487
815.038599	161.269327	49.613492
811.383862	152.545397	49.618497
807.848635	142.790426	49.623501
804.350586	142.520441	49.628506
800.688323	151.640348	49.633511
797.629898	141.553893	49.638516
793.780120	148.094943	49.643521
790.235448	142.746399	49.648525
786.979439	140.755667	49.653530
783.113415	152.668220	49.658535
779.770124	147.551512	49.663540
776.240766	157.012832	49.668545
773.311726	154.958934	49.673549
769.838886	148.691304	49.678554
765.956544	155.380503	49.683559
762.649909	142.921358	49.688564
758.766609	148.249670	49.693569
755.200177	142.570200	49.698573
751.858072	152.361190	49.703578
748.360929	149.189143	49.708583
745.047775	141.809657	49.713588
741.321347	152.535342	49.718593
737.712229	142.211639	49.723597
733.835834	144.655726	49.728602
730.556517	155.313302	49.733607
727.499519	134.315595	49.738612
723.990397	149.547379	49.743617
720.307230	149.193767	49.748621
716.813213	144.806878	49.753626
713.371411	144.584576	49.758631
710.130276	133.131592	49.763636
706.441164	150.252163	49.768641
702.885004	145.069926	49.773645
699.726790	135.751170	49.778650
695.464078	146.171707	49.783655
692.143416	137.713813	49.788660
688.963020	142.552074	49.793665
685.152411	145.361693	49.798669
682.141114	139.641789	49.803674
678.071957	150.257870	49.808679
674.611670	149.174422	49.813684
671.321677	149.747881	49.818689
668.038492	148.607072	49.823693
664.630240	140.095587	49.828698
661.121081	149.417078	49.833703
657.700985	144.607510	49.838708
653.645608	147.080512	49.843713
650.266359	148.497721	49.848717
646.588002	140.151512	49.853722
643.048728	155.041241	49.858727
639.887556	142.692321	49.863732
636.347767	142.838442	49.868737
632.436452	143.806556	49.873741
629.016543	140.204907	49.878746
625.446076	154.106043	49.883751
622.265250	153.242836	49.888756
618.906443	152.208461	49.893761
615.211099	147.971984	49.898765
611.879043	146.087524	49.903770
608.283685	151.053453	49.908775
605.151341	143.317735	49.913780
601.471026	143.226931	49.918785
597.651829	140.269366	49.923789
594.156666	129.614307	49.928794
590.522268	147.589999	49.933799
587.209012	134.300011	49.938804
583.751385	137.043688	49.943809
580.204229	146.704844	49.948813
576.713937	134.011468	49.953818
573.428303	143.283348	49.958823
569.700928	140.264956	49.963828
565.877437	137.967629	49.968833
562.770537	139.039197	49.973837
559.375422	134.590487	49.978842
555.413320	146.457449	49.983847
552.471328	132.643471	49.988852
548.613143	135.841139	49.993857
545.402635	145.016864	49.998861
541.977410	140.825199	50.003866
538.121423	144.894226	50.008871
534.767259	128.531719	50.013876
530.838351	141.635961	50.018881
527.402359	131.736337	50.023885
524.236048	140.297844	50.028890
520.542845	140.828471	50.033895
517.059648	132.671595	50.038900
513.569966	137.654542	50.043905
510.100818	144.027403	50.048909
506.404759	127.687354	50.053914
502.814038	144.152953	50.058919
500.001889	137.023127	50.063924
496.682575	139.694082	50.068929
492.819421	144.434678	50.073933
489.252577	129.155145	50.078938
485.161419	143.176865	50.083943
481.893124	135.523265	50.088948
478.521156	133.350493	50.093953
475.139089	134.551608	50.098957
472.067160	135.116868	50.103962
468.026992	146.730892	50.108967
464.496859	140.896240	50.113972
460.941655	143.655309	50.118977
457.510059	148.110063	50.123981
454.308861	134.015865	50.128986
450.457583	131.325719	50.133991
447.264464	136.613091	50.138996
444.014647	135.388850	50.144001
440.170078	129.774562	50.149005
436.517292	131.889269	50.154010
432.805237	139.600388	50.159015
429.503637	125.551114	50.164020
426.077620	135.479207	50.169025
422.348758	125.872501	50.174029
419.406636	133.467585	50.179034
415.769333	137.950912	50.184039
412.036521	135.627847	50.189044
408.365406	134.032826	50.194049
404.892350	133.637287	50.199053
401.774190	136.251283	50.204058
397.865361	142.069680	50.209063
394.368592	126.473898	50.214068
390.704385	145.592073	50.219073
387.308975	134.986271	50.224077
383.994376	134.418163	50.229082
380.484110	135.211357	50.234087
377.195868	120.066131	50.239092
373.287957	132.385133	50.244097
369.807591	143.812510	50.249101
366.548601	124.555361	50.254106
363.042857	139.063869	50.259111
359.481495	141.324223	50.264116
355.832644	138.931582	50.269121
351.978656	139.820543	50.274125
349.321564	130.277344	50.279130
345.609167	129.956005	50.284135
342.516781	126.700162	50.289140
338.735424	132.709538	50.294145
334.920925	124.012626	50.299149
331.828239	132.554741	50.304154
327.767398	135.737081	50.309159
324.362737	131.090604	50.314164
320.699730	135.570235	50.319169
317.062458	132.093858	50.324173
313.901576	127.342792	50.329178
310.622343	138.920262	50.334183
307.108471	122.764053	50.339188
303.715613	136.254266	50.344193
299.856657	135.218637	50.349197
296.294348	140.727581	50.354202
292.521838	142.394326	50.359207
289.289040	127.636584	50.364212
285.935344	128.609952	50.369217
282.610520	136.069824	50.374221
279.431105	128.804272	50.379226
275.355526	134.241064	50.384231
271.999082	132.902037	50.389236
268.366541	134.225043	50.394241
264.480159	138.467744	50.399245
261.396997	126.162318	50.404250
257.980914	145.454022	50.409255
254.565863	142.143800	50.414260
251.133537	133.084481	50.419265
247.123531	138.346493	50.424269
243.778887	130.050091	50.429274
239.970483	131.958186	50.434279
236.587819	133.923305	50.439284
233.630623	126.229408	50.444289
230.299695	133.257611	50.449293
226.845746	129.513342	50.454298
222.819636	115.841211	50.459303
219.595091	132.677820	50.464308
215.709465	136.482693	50.469313
211.733455	132.951361	50.474317
208.804021	134.596750	50.479322
205.206297	132.256622	50.484327
201.977248	133.523061	50.489332
198.741102	128.983972	50.494337
194.576421	133.683095	50.499341
191.409039	127.142493	50.504346
187.855642	136.792418	50.509351
184.196256	131.538372	50.514356
180.861851	139.360751	50.519361
177.345746	121.971036	50.524365
174.062551	129.078488	50.529370
170.557928	126.196283	50.534375
166.661066	134.781563	50.539380
163.343050	134.293452	50.544385
159.597611	132.811487	50.549389
156.672113	126.799384	50.554394
152.640054	128.321257	50.559399
149.401206	131.529084	50.564404
145.848041	124.539546	50.569409
142.055255	127.199033	50.574413
138.701426	139.287101	50.579418
134.968913	125.276670	50.584423
132.042634	123.006177	50.589428
128.661145	136.173064	50.594433
124.720480	129.034671	50.599437
121.508941	129.750429	50.604442
117.910794	132.748018	50.609447
114.232719	129.432014	50.614452
110.688255	129.568146	50.619457
107.198953	131.358182	50.624461
103.920460	123.775654	50.629466
99.893695	129.397745	50.634471
96.660704	127.321788	50.639476
93.359596	121.832306	50.644481
89.668711	130.406574	50.649485
86.151987	123.201216	50.654490
82.853215	131.918065	50.659495
79.095714	122.583880	50.664500
75.716987	131.709548	50.669505
72.091528	138.993767	50.674509
68.584268	117.996761	50.679514
65.398314	127.135464	50.684519
61.948085	132.231681	50.689524
58.310943	129.347762	50.694529
54.724549	128.707934	50.699533
51.162241	124.479920	50.704538
47.590834	129.353774	50.709543
44.282517	122.309635	50.714548
40.850948	124.090559	50.719553
36.908129	130.805814	50.724557
33.349530	122.801700	50.729562
30.120817	122.871197	50.734567
26.795746	128.293220	50.739572
23.241786	138.209484	50.744577
19.531678	129.907418	50.749581
16.321930	128.665238	50.754586
12.839557	124.638710	50.759591
9.530874	122.850258	50.764596
6.013356	129.428753	50.769601
1.875357	130.865232	50.774605