Thu Jun 16 11:01:19 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.595597	118.406347	0.000000
1.468733	115.606638	0.005005
1.174034	112.918523	0.010010
0.884101	101.092386	0.015014
0.804658	83.674596	0.020019
0.862615	85.079263	0.025024
0.221001	68.646720	0.030029
0.204448	69.761622	0.035034
0.318844	71.019734	0.040038
-0.295956	55.526200	0.045043
-0.471330	37.985608	0.050048
-0.712488	37.308195	0.055053
-1.362035	36.100927	0.060058
-1.408359	25.414881	0.065062
-1.503682	20.548514	0.070067
-1.644790	15.034854	0.075072
-2.128238	2.279398	0.080077
-2.680897	6.786498	0.085082
-2.811624	-0.386248	0.090086
-3.022307	-0.874151	0.095091
-3.591316	-3.241274	0.100096
-3.629059	-3.269523	0.105101
-3.824057	-6.737670	0.110106
-3.874284	-2.876127	0.115110
-4.431865	-11.685026	0.120115
-5.114396	-15.647254	0.125120
-5.397361	-7.640710	0.130125
-5.484226	-7.094669	0.135130
-5.510296	-4.345883	0.140134
-5.642714	-9.913749	0.145139
-5.411492	-14.303908	0.150144
-6.183321	3.541719	0.155149
-6.581754	-5.964326	0.160154
-6.610765	-5.473227	0.165158
-7.115966	4.839569	0.170163
-7.123273	-8.371520	0.175168
-7.524338	2.737362	0.180173
-8.464480	-9.241972	0.185178
-8.029023	-13.927216	0.190182
-8.539025	2.707974	0.195187
-8.683897	-0.929954	0.200192
-8.514941	-9.774871	0.205197
-8.360095	-1.715981	0.210202
-9.094323	-10.769055	0.215206
-9.916269	-4.242514	0.220211
-10.372515	-8.624422	0.225216
-10.257340	-7.278151	0.230221
-10.380186	-11.356948	0.235226
-10.008426	-0.424523	0.240230
-10.541190	-5.880057	0.245235
-10.410509	-4.371993	0.250240
-10.791654	-1.052218	0.255245
-11.553619	-7.707182	0.260250
-11.510050	-19.675648	0.265254
-12.529943	-1.901002	0.270259
-13.274748	-16.960702	0.275264
-12.612939	-12.631724	0.280269
-12.649565	-5.715955	0.285274
-13.014354	-11.506158	0.290278
-13.625977	-11.917342	0.295283
-13.431825	-16.425085	0.300288
-13.487431	-16.557715	0.305293
-13.431961	-2.441176	0.310298
-14.228785	-12.845811	0.315302
-14.693942	-5.946233	0.320307
-15.205405	-2.732678	0.325312
-14.834545	-13.150839	0.330317
-14.968936	-3.888132	0.335322
-15.319127	-8.131990	0.340326
-16.020567	-3.518126	0.345331
-16.552878	-4.197238	0.350336
-16.382057	-14.280263	0.355341
-16.517974	-9.736679	0.360346
-16.470553	-9.320067	0.365350
-16.924951	-8.482240	0.370355
-16.994384	-9.721744	0.375360
-17.495249	-6.890939	0.380365
-17.762386	-18.360269	0.385370
-17.961785	-15.456564	0.390374
-18.416378	-3.447212	0.395379
-18.359060	-3.640532	0.400384
-18.633063	-4.385813	0.405389
-19.496446	-2.780054	0.410394
-19.141223	-2.627502	0.415398
-19.639612	3.814297	0.420403
-19.444900	1.325396	0.425408
-19.620455	0.394654	0.430413
-20.938732	2.320154	0.435418
-21.274106	-2.296302	0.440422
-21.512110	0.925137	0.445427
-21.180047	-4.118004	0.450432
-21.189932	-3.830036	0.455437
-21.687724	-4.678716	0.460442
-21.440461	-5.912749	0.465446
-21.488805	-0.742093	0.470451
-21.921648	-10.483752	0.475456
-22.651050	-10.136557	0.480461
-23.316882	-3.164155	0.485466
-22.780272	-5.483149	0.490470
-23.299150	-3.785655	0.495475
-23.255689	-9.840930	0.500480
-23.911430	-4.407608	0.505485
-24.404990	-5.581161	0.510490
-24.440598	-8.837401	0.515494
-24.788826	1.238037	0.520499
-24.621618	-5.299882	0.525504
-24.501201	-8.396143	0.530509
-25.535715	1.917709	0.535514
-25.880629	-5.172083	0.540518
-25.882697	3.730379	0.545523
-25.842257	0.654535	0.550528
-25.979572	-0.025239	0.555533
-26.351564	3.544886	0.560538
-27.095238	-8.978825	0.565542
-27.466702	-8.444053	0.570547
-27.713096	5.585153	0.575552
-27.595822	-7.136092	0.580557
-27.726109	0.717072	0.585562
-27.477687	-4.843592	0.590566
-28.153615	-2.686265	0.595571
-28.716825	2.911613	0.600576
-28.982841	0.001052	0.605581
-29.342451	-2.394066	0.610586
-29.616075	8.142878	0.615590
-29.613962	-4.953555	0.620595
-29.623010	1.739437	0.625600
-29.689220	5.852624	0.630605
-30.452166	-2.062868	0.635610
-30.676374	5.208870	0.640614
-31.186154	4.026355	0.645619
-31.619524	2.473496	0.650624
-31.035423	-3.113642	0.655629
-31.369850	-1.781558	0.660634
-31.256785	-2.695875	0.665638
-31.637780	3.663877	0.670643
-32.869238	-11.054950	0.675648
-32.575730	2.647073	0.680653
-32.665229	1.452023	0.685658
-32.772928	-0.297608	0.690662
-33.258843	2.647731	0.695667
-34.038270	4.065099	0.700672
-34.027302	-10.299796	0.705677
-34.578809	4.446828	0.710682
-34.315247	-5.208970	0.715686
-34.242796	0.109532	0.720691
-34.688048	-3.248493	0.725696
-34.619228	-11.606775	0.730701
-35.516895	8.503027	0.735706
-35.832427	-9.510565	0.740710
-36.290711	3.048208	0.745715
-36.016770	-3.798180	0.750720
-35.907199	-13.166697	0.755725
-36.328502	6.651777	0.760730
-36.742849	-9.319934	0.765734
-37.326995	-2.004892	0.770739
-37.664935	2.431404	0.775744
-37.417410	-6.907433	0.780749
-37.718382	1.930778	0.785754
-37.696571	-4.889626	0.790758
-38.493452	-10.558792	0.795763
-39.298258	-1.338396	0.800768
-39.000096	-10.366653	0.805773
-39.285201	-8.942786	0.810778
-39.379349	-0.851528	0.815782
-39.434385	-14.942303	0.820787
-39.265455	-7.168881	0.825792
-39.554801	2.279256	0.830797
-40.581914	-6.472757	0.835802
-40.776127	-13.942799	0.840806
-40.704802	-1.487539	0.845811
-40.889235	-0.441084	0.850816
-41.631607	-6.209035	0.855821
-42.394493	6.643855	0.860826
-41.732573	-0.874655	0.865830
-41.973684	6.457785	0.870835
-42.712308	-12.013278	0.875840
-42.380304	2.148713	0.880845
-42.977966	-0.394699	0.885850
-42.379646	-9.684373	0.890854
-43.179435	-10.913859	0.895859
-44.118071	-10.170320	0.900864
-43.828678	-9.761934	0.905869
-44.101753	12.443232	0.910874
-44.118604	-5.479835	0.915878
-44.178199	-0.512815	0.920883
-44.931476	9.305888	0.925888
-44.984033	-8.217056	0.930893
-45.400805	2.531673	0.935898
-45.318804	11.273842	0.940902
-45.925738	-1.178651	0.945907
-46.949440	-8.967382	0.950912
-46.087429	-9.634245	0.955917
-46.927138	-2.132637	0.960922
-46.740391	-3.149300	0.965926
-47.178457	-4.239191	0.970931
-47.369431	0.976051	0.975936
-47.089173	-2.682513	0.980941
-47.963701	0.367501	0.985946
-48.401562	4.725309	0.990950
-48.852417	-3.191248	0.995955
-49.308598	5.594976	1.000960
-49.288901	-1.539389	1.005965
-49.056025	1.063607	1.010970
-48.953918	-0.845099	1.015974
-48.819091	-5.022220	1.020979
-49.412756	-4.318035	1.025984
-49.641706	0.267071	1.030989
-50.328038	-5.969666	1.035994
-50.664674	-4.747315	1.040998
-51.295183	4.485418	1.046003
-51.653337	7.947501	1.051008
-51.651412	-4.542476	1.056013
-51.983963	5.516265	1.061018
-52.069625	2.678299	1.066022
-52.128824	-0.941032	1.071027
-52.000613	4.581247	1.076032
-51.839050	-17.416865	1.081037
-52.715322	-3.696729	1.086042
-53.163565	5.863203	1.091046
-53.505338	-3.663053	1.096051
-53.803086	-3.181206	1.101056
-53.326940	3.821770	1.106061
-54.423582	0.502148	1.111066
-54.934570	-6.730370	1.116070
-55.117525	-8.859313	1.121075
-54.736356	7.163540	1.126080
-54.995610	-1.775260	1.131085
-55.484067	1.602404	1.136090
-55.237888	4.812287	1.141094
-55.282132	-12.834847	1.146099
-55.863599	0.425778	1.151104
-56.757227	-0.117849	1.156109
-56.706942	-3.737813	1.161114
-56.650851	-7.845786	1.166118
-57.012957	1.941904	1.171123
-57.775503	4.795244	1.176128
-57.964338	-12.710102	1.181133
-58.370615	-5.348792	1.186138
-58.154260	-2.343225	1.191142
-58.470471	-0.723914	1.196147
-58.828430	7.899775	1.201152
-58.416582	1.716332	1.206157
-58.683457	-6.213758	1.211162
-59.224491	-0.503629	1.216166
-59.972224	7.728208	1.221171
-60.505526	-0.827609	1.226176
-60.268445	4.649743	1.231181
-60.382021	5.439138	1.236186
-60.080190	1.022803	1.241190
-60.799397	-8.392630	1.246195
-61.238231	-6.346799	1.251200
-61.579446	-13.815529	1.256205
-61.857068	8.608896	1.261210
-61.606189	-6.503388	1.266214
-61.965491	-9.577681	1.271219
-61.985396	-1.456768	1.276224
-62.985761	1.886920	1.281229
-63.594658	-0.460977	1.286234
-63.652007	-11.671680	1.291238
-63.682930	-9.228511	1.296243
-63.980051	-4.555980	1.301248
-63.677345	-5.833706	1.306253
-63.724209	2.546190	1.311258
-63.674092	-12.009454	1.316262
-64.211893	-7.018055	1.321267
-64.736267	-10.224687	1.326272
-64.702451	-4.874845	1.331277
-65.603524	2.736252	1.336282
-66.442070	0.950455	1.341286
-66.422118	-4.015649	1.346291
-66.387959	-2.063183	1.351296
-66.432274	-1.379253	1.356301
-66.842394	-1.269698	1.361306
-66.782831	-7.764962	1.366310
-66.655907	-4.465032	1.371315
-67.001495	0.781977	1.376320
-67.683503	-13.177254	1.381325
-67.979156	-8.161555	1.386330
-67.921900	-5.730098	1.391334
-68.018385	-7.817592	1.396339
-69.054432	0.745322	1.401344
-69.424654	-3.017641	1.406349
-69.273262	-2.597003	1.411354
-69.824712	-9.177243	1.416358
-69.774514	-2.125874	1.421363
-69.971739	-12.648239	1.426368
-69.930296	-12.785662	1.431373
-69.753612	0.129367	1.436378
-70.152808	-13.103263	1.441382
-70.703017	-16.766530	1.446387
-71.265825	0.900313	1.451392
-71.327335	-11.671708	1.456397
-71.528812	-3.605432	1.461402
-72.639041	-4.056138	1.466406
-72.420184	-15.415481	1.471411
-72.779497	-3.738063	1.476416
-72.838727	-9.216210	1.481421
-73.259266	-4.480564	1.486426
-73.207080	-6.514892	1.491430
-73.150810	-13.777624	1.496435
-73.043073	-3.145184	1.501440
-73.537710	-12.376054	1.506445
-74.365271	-3.899392	1.511450
-74.440434	-13.040463	1.516454
-74.209430	-14.364445	1.521459
-75.102992	-1.757413	1.526464
-75.695290	-16.726581	1.531469
-75.977346	-9.601755	1.536474
-75.714084	-8.991745	1.541478
-75.894926	-10.771606	1.546483
-76.460973	-4.150918	1.551488
-76.206648	-9.815746	1.556493
-76.591308	-1.904958	1.561498
-76.544956	-10.121015	1.566502
-76.919718	-10.495870	1.571507
-77.833625	-1.555571	1.576512
-77.661517	-7.926190	1.581517
-77.929553	2.248653	1.586522
-77.960741	-3.211243	1.591526
-77.966139	-8.119883	1.596531
-79.231902	-3.261707	1.601536
-79.395721	-9.096266	1.606541
-79.773424	-4.046781	1.611546
-79.537316	1.585418	1.616550
-79.237665	-6.929399	1.621555
-79.439771	7.216589	1.626560
-79.710586	-6.196291	1.631565
-80.850661	0.946638	1.636570
-80.907233	-9.193608	1.641574
-81.095613	-5.614369	1.646579
-81.714603	1.994501	1.651584
-81.410660	-15.585178	1.656589
-81.588107	-5.561848	1.661594
-81.433183	0.357135	1.666598
-81.925487	-6.617725	1.671603
-82.750518	-3.511568	1.676608
-82.553919	-3.535633	1.681613
-82.754082	-14.379020	1.686618
-83.053156	-14.686376	1.691622
-83.559602	-9.813907	1.696627
-84.157279	-1.248666	1.701632
-84.051913	-10.043508	1.706637
-84.499136	-7.656824	1.711642
-84.564294	-5.106384	1.716646
-84.348049	-16.364469	1.721651
-84.710838	-12.804451	1.726656
-84.716788	-14.319526	1.731661
-85.466765	0.037756	1.736666
-85.909361	-11.931250	1.741670
-85.553261	-17.472415	1.746675
-86.128662	-10.370827	1.751680
-87.044901	-14.759961	1.756685
-87.040697	-8.969575	1.761690
-87.460324	-12.273326	1.766694
-87.500079	-14.017708	1.771699
-87.615758	-4.900357	1.776704
-87.523624	-13.782785	1.781709
-87.803888	-15.735133	1.786714
-87.586309	-13.042602	1.791718
-88.036585	-14.964582	1.796723
-88.987874	-11.288159	1.801728
-89.033569	-17.452599	1.806733
-89.649537	-12.779757	1.811738
-89.266834	-9.429667	1.816742
-88.961363	-13.686386	1.821747
-90.618689	-8.515776	1.826752
-90.698207	-10.407090	1.831757
-90.900982	-8.648090	1.836762
-90.881155	-17.583083	1.841766
-90.837645	-10.953046	1.846771
-91.180610	-8.328378	1.851776
-91.112627	-12.575639	1.856781
-91.473971	-7.348817	1.861786
-91.892657	-11.103075	1.866790
-92.702514	-7.906297	1.871795
-92.774207	-4.714912	1.876800
-92.611958	-7.035076	1.881805
-93.190802	-10.338556	1.886810
-92.892770	-11.323892	1.891814
-92.801139	-24.879526	1.896819
-93.983648	-9.867825	1.901824
-94.360441	-8.065067	1.906829
-94.530846	-4.538619	1.911834
-94.395774	-6.584870	1.916838
-94.511574	-11.657671	1.921843
-94.762849	-13.417208	1.926848
-95.283185	-21.957590	1.931853
-95.747601	-10.412859	1.936858
-96.012605	-19.169467	1.941862
-96.158462	-19.600108	1.946867
-96.366924	-9.854099	1.951872
-96.043910	-23.455771	1.956877
-96.516711	-13.901857	1.961882
-96.952251	-11.591882	1.966886
-96.879156	-8.570139	1.971891
-97.187800	-9.358919	1.976896
-97.329018	-9.467929	1.981901
-98.045790	-10.506817	1.986906
-98.673481	-4.318893	1.991910
-98.613011	-9.329278	1.996915
-99.190570	-12.589205	2.006912
-98.243671	-7.178363	2.016909
-97.798874	-14.635559	2.026906
-97.457374	-14.998281	2.036902
-97.032579	-14.223299	2.046899
-96.643652	-19.571553	2.056896
-96.420040	-14.404332	2.066893
-95.194124	-7.786143	2.076890
-94.795716	-13.735607	2.086886
-94.719769	-16.478091	2.096883
-93.932916	-10.742632	2.106880
-93.446613	-12.279278	2.116877
-92.927072	-9.783807	2.126874
-91.925696	-10.710323	2.136870
-91.666854	-6.439715	2.146867
-91.539087	-6.745726	2.156864
-91.698872	-9.390774	2.166861
-90.751881	-11.095524	2.176858
-89.490645	-15.694245	2.186854
-88.958355	-13.619706	2.196851
-89.038827	-3.334737	2.206848
-88.819433	-3.920869	2.216845
-87.465345	-13.515991	2.226842
-87.233146	-7.583065	2.236838
-86.888260	-14.643002	2.246835
-86.929691	-12.957313	2.256832
-85.928255	-8.802030	2.266829
-85.471216	-3.082584	2.276826
-85.310268	-12.058473	2.286822
-84.315246	-13.211132	2.296819
-84.062612	-10.074918	2.306816
-83.004628	-6.139874	2.316813
-82.581827	-1.969459	2.326810
-82.645241	-11.454765	2.336806
-82.297480	-3.017466	2.346803
-81.356298	-5.760812	2.356800
-80.872864	-1.297510	2.366797
-80.508834	-1.506254	2.376794
-79.427683	-0.640413	2.386790
-79.490086	1.458333	2.396787
-79.207228	0.409550	2.406784
-78.289657	6.266940	2.416781
-77.994779	0.446549	2.426778
-77.373691	1.470267	2.436774
-76.530471	5.760412	2.446771
-76.248246	-1.683601	2.456768
-76.438343	3.497823	2.466765
-75.369419	1.809321	2.476762
-74.816168	-2.848662	2.486758
-74.530511	-2.687068	2.496755
-73.410706	5.268216	2.506752
-73.141529	7.681794	2.516749
-73.088446	3.438128	2.526746
-72.692952	-0.260018	2.536742
-71.867459	-4.274204	2.546739
-71.553669	-0.652963	2.556736
-71.130771	4.694002	2.566733
-70.316961	0.792181	2.576730
-70.102542	0.740726	2.586726
-69.248611	-1.864526	2.596723
-68.748509	1.397926	2.606720
-68.651524	-2.163118	2.616717
-67.481197	-0.616309	2.626714
-66.977498	-1.197025	2.636710
-66.859749	-5.335459	2.646707
-66.879700	-5.482963	2.656704
-65.828709	-3.910602	2.666701
-65.600958	-0.792301	2.676698
-64.553127	4.619997	2.686694
-64.045854	1.196999	2.696691
-64.255991	3.439932	2.706688
-63.760342	2.269597	2.716685
-62.590262	-4.078359	2.726682
-62.571797	-5.789916	2.736678
-61.587630	-5.014576	2.746675
-60.758952	-0.972927	2.756672
-60.939166	-2.471968	2.766669
-60.811056	0.577160	2.776666
-60.148178	-0.499215	2.786662
-59.493572	-0.240254	2.796659
-58.726451	3.958653	2.806656
-57.974681	3.258359	2.816653
-57.808931	-0.794120	2.826650
-57.763698	-2.100215	2.836646
-56.876840	-1.695366	2.846643
-56.411860	1.072129	2.856640
-55.570046	5.090076	2.866637
-55.058062	-2.550452	2.876634
-54.793403	4.191950	2.886630
-54.418375	1.166122	2.896627
-54.126425	-1.115599	2.906624
-53.047294	3.704777	2.916621
-52.604462	-0.599648	2.926618
-52.346729	0.641580	2.936614
-52.172120	0.136491	2.946611
-51.356928	2.917426	2.956608
-50.844084	1.353033	2.966605
-49.776643	2.795253	2.976602
-49.584188	-0.743243	2.986598
-49.479082	1.329300	2.996595
-49.343831	7.654362	3.006592
-48.579535	-3.640236	3.016589
-47.895057	-0.567289	3.026586
-46.800589	-3.563059	3.036582
-46.370305	-2.592457	3.046579
-46.154866	-2.863568	3.056576
-46.079124	-5.264442	3.066573
-45.806470	-4.852020	3.076570
-44.989898	-3.155963	3.086566
-44.410842	-3.876261	3.096563
-43.613567	-3.335846	3.106560
-43.232722	-4.897536	3.116557
-42.998092	1.284958	3.126554
-42.091522	-3.737039	3.136550
-41.497677	1.314774	3.146547
-41.491411	2.727161	3.156544
-40.893873	3.467821	3.166541
-40.226316	3.740102	3.176538
-39.915249	3.894683	3.186534
-39.122649	-0.613100	3.196531
-38.552125	0.742779	3.206528
-38.406666	2.176464	3.216525
-38.217946	3.996291	3.226522
-37.466354	-7.179595	3.236518
-36.671864	6.910877	3.246515
-36.127866	5.900084	3.256512
-35.650494	4.061514	3.266509
-35.230656	-0.862558	3.276506
-35.099771	-2.627959	3.286502
-34.009616	0.395033	3.296499
-33.626281	1.173316	3.306496
-33.615110	6.037439	3.316493
-32.653138	1.327170	3.326490
-32.174672	7.126258	3.336486
-32.126473	7.417975	3.346483
-30.855528	2.528772	3.356480
-30.320910	2.634801	3.366477
-30.309804	6.317184	3.376474
-30.190442	4.092731	3.386470
-28.987115	2.611587	3.396467
-28.508971	7.954170	3.406464
-28.577088	8.119806	3.416461
-28.195093	-0.575000	3.426458
-27.297498	-3.722208	3.436454
-26.969016	4.811143	3.446451
-25.775899	0.109100	3.456448
-25.613842	11.779937	3.466445
-25.450528	9.703204	3.476442
-25.151169	1.551859	3.486438
-24.303140	-2.652495	3.496435
-23.666565	1.287755	3.506432
-22.872077	-1.964158	3.516429
-22.666436	1.290314	3.526426
-22.102541	3.650101	3.536422
-22.012437	-0.968725	3.546419
-21.400341	-3.617325	3.556416
-20.772447	-5.232437	3.566413
-20.396893	-4.303265	3.576410
-19.306948	-5.939619	3.586406
-18.850135	3.914295	3.596403
-19.274090	6.102379	3.606400
-18.489863	4.183316	3.616397
-17.445648	6.871189	3.626394
-17.332709	-3.054494	3.636390
-16.763620	2.986889	3.646387
-15.737458	5.835695	3.656384
-15.568015	5.530650	3.666381
-15.523886	1.592950	3.676378
-15.145758	-3.119655	3.686374
-14.261913	-4.857128	3.696371
-13.875287	0.285833	3.706368
-13.005243	-0.058345	3.716365
-12.747194	-4.966049	3.726362
-12.370458	-2.920319	3.736358
-11.424135	-6.466695	3.746355
-11.181456	2.792445	3.756352
-11.038280	6.120016	3.766349
-9.917868	-3.174275	3.776346
-9.481928	3.772402	3.786342
-9.236489	1.972214	3.796339
-9.088788	1.647204	3.806336
-8.181760	-1.717098	3.816333
-7.938206	-0.977696	3.826330
-6.956678	-1.647353	3.836326
-6.286748	1.311790	3.846323
-6.109820	4.086446	3.856320
-6.058301	0.958950	3.866317
-5.632517	-3.421384	3.876314
-4.999528	-4.025043	3.886310
-3.837630	8.074913	3.896307
-3.671551	20.086921	3.906304
-3.529132	23.931586	3.916301
-2.847521	21.378226	3.926298
-2.825007	30.506534	3.936294
-2.280266	44.380757	3.946291
-1.680558	64.289320	3.956288
-1.067980	76.385779	3.966285
-0.442819	99.034145	3.976282
-0.081227	106.460387	3.986278
0.000000	120.787462	3.991283
0.719447	106.281887	3.996288
0.210631	129.397008	4.001293
0.754170	125.000478	4.006298
0.751962	139.551585	4.011302
1.068294	146.258151	4.016307
1.368054	142.265839	4.021312
0.878069	150.593170	4.026317
1.268247	140.050465	4.031322
0.962116	151.808992	4.036326
1.178837	157.251689	4.041331
1.334769	144.174296	4.046336
1.015635	152.295223	4.051341
1.251749	141.783602	4.056346
1.253940	149.030325	4.061350
1.146355	155.707410	4.066355
1.150600	135.222183	4.071360
1.295702	149.105335	4.076365
1.089123	137.917992	4.081370
1.261936	144.984786	4.086374
0.932743	142.767323	4.091379
1.276940	144.981898	4.096384
1.231739	144.103199	4.101389
1.216130	146.667182	4.106394
1.319837	146.534561	4.111398
1.243520	139.407116	4.116403
1.271322	150.053868	4.121408
1.268472	154.706918	4.126413
1.237655	151.856800	4.131418
1.492991	148.670731	4.136422
1.634331	152.587667	4.141427
1.447033	139.681243	4.146432
1.113068	138.299974	4.151437
1.236311	143.737693	4.156442
1.463512	146.731340	4.161446
1.222603	154.627825	4.166451
1.394438	151.665688	4.171456
1.156748	153.724860	4.176461
1.361769	147.481128	4.181466
1.230465	151.727641	4.186470
1.225291	162.780980	4.191475
1.427574	149.813616	4.196480
1.433597	156.690052	4.201485
1.531050	163.796537	4.206490
1.044077	154.131588	4.211494
1.178228	156.151407	4.216499
1.331402	142.777423	4.221504
1.191647	160.469447	4.226509
1.310742	164.837657	4.231514
1.766016	173.326549	4.236518
1.584776	188.649566	4.241523
1.736703	174.926819	4.246528
1.659679	187.414746	4.251533
1.888839	180.086152	4.256538
1.323579	164.343209	4.261542
1.627741	178.939713	4.266547
2.128233	174.869331	4.271552
1.362391	170.167594	4.276557
1.558081	174.544656	4.281562
1.990648	172.676714	4.286566
1.656879	178.990159	4.291571
1.959112	166.454747	4.296576
1.611682	169.806672	4.301581
1.847804	167.916935	4.306586
1.645705	160.491121	4.311590
1.633712	162.691953	4.316595
1.777640	169.721900	4.321600
1.937832	172.572231	4.326605
1.722188	174.158266	4.331610
2.019436	178.130043	4.336614
1.667531	176.111369	4.341619
1.926133	180.767192	4.346624
1.583676	177.862420	4.351629
2.081142	178.376221	4.356634
2.270406	178.743352	4.361638
1.701637	166.717103	4.366643
1.920558	159.235818	4.371648
1.820511	169.517776	4.376653
1.873253	180.742883	4.381658
2.005774	181.396808	4.386662
1.656699	186.601641	4.391667
1.914452	171.120945	4.396672
2.000018	176.096097	4.401677
1.612698	181.697427	4.406682
1.720132	174.959570	4.411686
1.721842	191.248370	4.416691
1.777887	179.245131	4.421696
1.742434	182.140425	4.426701
2.094064	178.850041	4.431706
1.782025	179.735479	4.436710
1.616128	187.478509	4.441715
1.925063	189.408084	4.446720
2.221840	204.643141	4.451725
2.363419	195.730710	4.456730
2.542953	197.411654	4.461734
2.204618	186.022204	4.466739
1.970964	176.529062	4.471744
1.871107	187.162606	4.476749
2.351691	195.031427	4.481754
2.603338	199.036397	4.486758
1.867373	185.191838	4.491763
2.053307	185.169045	4.496768
2.546848	206.659234	4.501773
2.775131	198.104302	4.506778
2.060635	184.662357	4.511782
1.987883	182.364527	4.516787
2.264837	175.840358	4.521792
1.815832	189.534349	4.526797
2.234536	191.086780	4.531802
2.703313	205.976831	4.536806
2.498448	207.535734	4.541811
2.464632	199.958474	4.546816
2.397370	195.416428	4.551821
2.195145	185.941961	4.556826
2.518221	191.385937	4.561830
2.335298	194.551550	4.566835
2.291116	184.773943	4.571840
2.427699	202.294068	4.576845
2.624904	204.697500	4.581850
2.659631	202.613644	4.586854
2.659752	199.247374	4.591859
2.133783	179.602052	4.596864
2.450191	195.148267	4.601869
2.219965	203.481927	4.606874
2.652339	199.989468	4.611878
2.336913	210.480778	4.616883
2.343097	211.038184	4.621888
2.657027	210.837575	4.626893
2.701821	203.731519	4.631898
2.541407	199.328776	4.636902
2.897397	216.610909	4.641907
2.900308	204.223095	4.646912
2.552934	196.616069	4.651917
2.441984	192.404929	4.656922
2.627902	194.005105	4.661926
2.798710	218.498812	4.666931
2.926027	196.984715	4.671936
2.605505	196.651594	4.676941
2.357132	190.275895	4.681946
2.601600	197.483390	4.686950
2.777342	211.305203	4.691955
2.927389	205.548021	4.696960
2.579397	212.306001	4.701965
2.546407	222.980312	4.706970
2.798909	213.858149	4.711974
2.650551	218.046234	4.716979
2.881218	212.593197	4.721984
2.812338	211.462695	4.726989
3.022599	211.350348	4.731994
3.040301	213.958262	4.736998
2.828525	215.758433	4.742003
2.847098	194.027414	4.747008
2.498943	202.951378	4.752013
2.894448	216.314339	4.757018
2.677229	205.258535	4.762022
2.768796	211.693585	4.767027
2.906683	209.972795	4.772032
2.945864	212.969214	4.777037
2.979723	207.724111	4.782042
3.136690	211.625260	4.787046
2.738238	220.980677	4.792051
3.067358	204.160261	4.797056
2.951912	223.706006	4.802061
2.758601	215.431465	4.807066
2.844362	211.478842	4.812070
2.557138	216.327777	4.817075
2.620936	210.802183	4.822080
2.677990	218.372930	4.827085
2.949160	210.061882	4.832090
2.990394	218.261010	4.837094
2.719333	228.995584	4.842099
3.321149	234.149636	4.847104
3.415309	240.492718	4.852109
3.251703	233.890193	4.857114
2.849864	226.635670	4.862118
3.196539	230.856880	4.867123
3.361666	227.510590	4.872128
2.945443	236.932585	4.877133
3.102532	231.058311	4.882138
3.177562	232.813256	4.887142
3.133129	244.198011	4.892147
3.321156	238.767501	4.897152
3.414299	240.576772	4.902157
3.261069	238.397300	4.907162
3.675400	245.301400	4.912166
3.127582	229.019713	4.917171
3.182396	225.275726	4.922176
3.230140	233.843939	4.927181
3.341006	241.091391	4.932186
3.417866	242.313299	4.937190
3.196250	251.346010	4.942195
3.135011	249.828600	4.947200
3.433286	242.973838	4.952205
3.724280	242.038489	4.957210
3.439272	243.526487	4.962214
3.410575	243.859497	4.967219
3.517074	233.424875	4.972224
3.341509	232.153168	4.977229
3.385286	242.255828	4.982234
3.533010	234.583733	4.987238
3.428168	246.375362	4.992243
3.514234	235.565577	4.997248
3.632132	247.506953	5.002253
3.432754	231.159491	5.007258
3.645008	231.225873	5.012262
3.145337	236.953422	5.017267
3.403483	232.071784	5.022272
3.404448	237.339341	5.027277
3.692136	238.213769	5.032282
3.664505	229.577202	5.037286
3.385360	241.687383	5.042291
3.300894	231.558286	5.047296
3.444570	246.644660	5.052301
2.844239	246.624444	5.057306
3.542205	240.383460	5.062310
3.091675	253.188386	5.067315
3.563168	245.421147	5.072320
3.725421	268.491969	5.077325
3.691866	268.511270	5.082330
3.694321	267.684178	5.087334
3.715625	264.834600	5.092339
3.641017	275.899792	5.097344
3.746119	275.894501	5.102349
3.847139	266.727592	5.107354
3.839715	262.324112	5.112358
3.803660	279.879960	5.117363
3.728889	274.564589	5.122368
3.739145	280.461920	5.127373
3.703075	276.299548	5.132378
3.606982	268.758394	5.137382
3.616409	272.395968	5.142387
3.944651	268.737204	5.147392
4.163792	274.995619	5.152397
3.904973	268.137710	5.157402
3.930050	268.845010	5.162406
3.822577	267.996129	5.167411
4.165057	265.148030	5.172416
4.029585	267.394638	5.177421
3.845380	265.784490	5.182426
4.048427	268.291837	5.187430
3.571356	269.510384	5.192435
3.776010	269.261636	5.197440
3.787493	267.225810	5.202445
3.488660	263.445154	5.207450
3.898366	260.731265	5.212454
3.798852	270.523479	5.217459
4.028928	268.526407	5.222464
3.875990	261.107611	5.227469
3.809801	272.204260	5.232474
4.280094	268.816803	5.237478
3.932224	278.584855	5.242483
3.904877	277.190389	5.247488
3.588860	281.860506	5.252493
4.060829	297.034442	5.257498
4.017543	301.564981	5.262502
4.099041	306.950958	5.267507
4.060043	300.189793	5.272512
4.256877	299.640944	5.277517
3.970782	303.414970	5.282522
4.286633	298.709147	5.287526
4.083391	298.765962	5.292531
4.288178	298.636169	5.297536
4.224071	293.790207	5.302541
3.891377	304.862457	5.307546
4.284513	302.956818	5.312550
4.284159	300.631122	5.317555
4.103290	292.048356	5.322560
4.328528	304.415492	5.327565
4.003841	303.994858	5.332570
4.198015	299.483172	5.337574
4.072384	314.955368	5.342579
4.113298	303.177888	5.347584
4.337363	313.167238	5.352589
4.482023	322.608369	5.357594
4.445614	324.713717	5.362598
4.190697	323.132513	5.367603
4.791292	332.382873	5.372608
4.820806	321.572311	5.377613
4.491310	314.368337	5.382618
4.280396	302.068858	5.387622
4.316328	308.710552	5.392627
4.499046	303.012159	5.397632
4.480736	313.505146	5.402637
4.580069	310.092366	5.407642
4.590022	296.305763	5.412646
4.345495	306.158763	5.417651
4.642043	307.680390	5.422656
4.598818	305.725519	5.427661
4.399594	303.529666	5.432666
4.448854	307.882427	5.437670
4.546595	317.433318	5.442675
4.519521	325.217897	5.447680
4.903187	328.070985	5.452685
4.878067	322.983179	5.457690
4.431186	315.864111	5.462694
4.494289	312.032706	5.467699
4.789434	322.393295	5.472704
4.806927	326.918335	5.477709
4.683485	329.801561	5.482714
4.869205	312.521709	5.487718
4.836593	305.036046	5.492723
4.591187	310.786518	5.497728
4.782341	297.422894	5.502733
4.579360	307.953303	5.507738
4.761184	313.842122	5.512742
4.818997	336.568932	5.517747
4.718919	325.155491	5.522752
4.564956	324.403574	5.527757
4.581834	332.737605	5.532762
4.949910	331.395087	5.537766
4.811659	335.934226	5.542771
4.887794	339.213426	5.547776
5.009820	328.595634	5.552781
4.959442	336.518438	5.557786
5.034411	337.727939	5.562790
5.165201	328.857762	5.567795
5.090298	323.741779	5.572800
4.760940	318.565938	5.577805
4.702553	326.474967	5.582810
4.959149	332.256628	5.587814
4.921585	335.791883	5.592819
4.839867	335.246448	5.597824
5.248378	328.593630	5.602829
4.951255	331.488985	5.607834
5.131397	338.008006	5.612838
5.012087	346.780484	5.617843
5.086021	333.891496	5.622848
5.262426	338.399649	5.627853
4.901997	347.368738	5.632858
5.055538	328.326377	5.637862
4.923431	334.426118	5.642867
5.207377	332.662827	5.647872
5.311232	335.827838	5.652877
4.848348	354.232701	5.657882
5.317018	338.920704	5.662886
4.767909	344.091858	5.667891
4.715134	343.816889	5.672896
4.574002	344.726379	5.677901
4.796375	334.579062	5.682906
4.713851	344.527548	5.687910
5.223714	345.774785	5.692915
5.562396	344.847727	5.697920
5.133460	353.700777	5.702925
4.730588	348.325164	5.707930
5.348353	355.542567	5.712934
5.300955	374.617228	5.717939
5.451325	369.973360	5.722944
5.280122	360.490796	5.727949
5.440092	360.805158	5.732954
5.187950	352.139231	5.737958
5.231114	364.130537	5.742963
5.555785	370.044310	5.747968
5.950311	357.725824	5.752973
5.205235	343.277671	5.757978
5.458543	340.932837	5.762982
4.916681	348.552411	5.767987
5.375134	352.876825	5.772992
5.640152	368.921337	5.777997
5.084149	372.385219	5.783002
5.442085	360.830454	5.788006
5.357016	369.198420	5.793011
5.377786	359.485834	5.798016
5.299505	367.161595	5.803021
5.473656	369.329722	5.808026
5.826783	364.101750	5.813030
5.673313	367.719010	5.818035
5.690466	363.805212	5.823040
5.746530	364.243984	5.828045
5.172586	364.837286	5.833050
5.505022	369.856448	5.838054
5.542517	372.211717	5.843059
5.589331	365.882660	5.848064
5.631791	361.355481	5.853069
5.536791	377.735440	5.858074
5.877429	362.975346	5.863078
5.912529	368.640118	5.868083
5.912056	367.133569	5.873088
5.904435	369.422992	5.878093
5.848688	377.488177	5.883098
5.614165	357.154087	5.888102
5.437103	356.548247	5.893107
5.412421	358.789976	5.898112
5.522382	361.017347	5.903117
5.466141	369.189848	5.908122
5.821191	366.484183	5.913126
5.614515	375.578527	5.918131
5.609623	363.822974	5.923136
5.686205	360.990486	5.928141
5.299407	366.427337	5.933146
5.844782	359.593051	5.938150
5.416328	372.511335	5.943155
5.944667	369.429270	5.948160
5.927954	360.554447	5.953165
5.679594	389.642541	5.958170
5.981967	378.504295	5.963174
6.166821	382.042265	5.968179
5.752625	381.989906	5.973184
5.949866	379.867921	5.978189
6.073407	382.622240	5.983194
5.778411	372.701182	5.988198
5.742989	379.704236	5.993203
5.865097	391.024483	5.998208
5.956426	391.427239	6.003213
6.125454	401.997355	6.008218
6.090039	402.276232	6.013222
6.225719	390.473552	6.018227
5.916611	383.390680	6.023232
6.011272	371.070439	6.028237
5.602384	372.888109	6.033242
5.980804	387.529760	6.038246
6.037784	388.179111	6.043251
6.249360	385.120289	6.048256
6.112530	370.559159	6.053261
5.985315	368.606224	6.058266
6.167856	359.341240	6.063270
6.147878	360.210583	6.068275
6.039407	363.110579	6.073280
5.966304	364.858351	6.078285
5.647751	374.323581	6.083290
5.727708	368.615114	6.088294
5.546158	373.531972	6.093299
5.936672	379.441081	6.098304
6.596073	393.602514	6.103309
6.054849	380.745991	6.108314
6.362637	371.954862	6.113318
6.121837	371.682454	6.118323
6.127133	367.190716	6.123328
6.401784	373.436938	6.128333
5.973756	371.320028	6.133338
6.210581	363.258055	6.138342
6.354929	368.378445	6.143347
6.138533	366.620196	6.148352
6.354850	363.412315	6.153357
5.697702	356.101366	6.158362
5.551440	353.592400	6.163366
5.712679	364.132799	6.168371
5.697772	367.551455	6.173376
5.803911	368.535016	6.178381
5.721659	368.478606	6.183386
6.129053	364.479992	6.188390
5.803031	373.111532	6.193395
5.940906	370.452906	6.198400
6.079142	369.167607	6.203405
5.905709	371.696345	6.208410
6.203276	376.793389	6.213414
6.229799	373.711187	6.218419
6.117981	375.606930	6.223424
6.067256	377.020016	6.228429
5.932529	369.822994	6.233434
6.242982	365.627205	6.238438
6.072110	373.548731	6.243443
5.854038	370.173890	6.248448
6.090345	367.691870	6.253453
5.766137	387.004078	6.258458
5.977097	366.014385	6.263462
6.218387	371.970153	6.268467
5.958311	383.957230	6.273472
6.096470	363.283431	6.278477
5.878800	374.008296	6.283482
6.165456	360.465066	6.288486
5.875598	356.827632	6.293491
6.139171	367.388906	6.298496
5.987314	346.819588	6.303501
5.625328	345.996190	6.308506
6.018151	362.475561	6.313510
5.979848	362.973436	6.318515
6.171187	362.439897	6.323520
5.800920	347.945188	6.328525
5.764908	356.162088	6.333530
5.918302	366.120435	6.338534
5.723336	377.615109	6.343539
5.925980	371.782778	6.348544
5.979304	367.421713	6.353549
5.919101	371.685541	6.358554
5.691394	374.596760	6.363558
5.868373	366.405276	6.368563
5.758346	370.702889	6.373568
5.970613	367.556942	6.378573
5.856293	369.726078	6.383578
6.068548	366.597595	6.388582
6.044682	376.236002	6.393587
5.868416	363.873230	6.398592
5.808674	367.119347	6.403597
5.903713	373.730090	6.408602
5.942549	374.053916	6.413606
6.146758	375.123970	6.418611
5.973883	380.323919	6.423616
6.056598	372.675917	6.428621
5.746876	372.277373	6.433626
6.020111	377.152517	6.438630
6.128249	359.759351	6.443635
5.635033	372.003766	6.448640
6.228795	376.587882	6.453645
5.654979	381.140318	6.458650
6.031657	376.041043	6.463654
6.438352	367.027578	6.468659
5.948978	369.292535	6.473664
6.197425	368.240692	6.478669
5.693707	375.933788	6.483674
5.996851	371.621411	6.488678
6.006184	367.407017	6.493683
6.077263	374.830401	6.498688
6.272498	375.428885	6.503693
6.052412	371.908761	6.508698
6.103756	371.185557	6.513702
6.176764	375.046659	6.518707
6.094142	367.557590	6.523712
6.272275	365.291867	6.528717
5.775915	356.720360	6.533722
5.788460	347.959786	6.538726
6.044593	355.405161	6.543731
5.637509	347.775273	6.548736
5.961133	365.186933	6.553741
5.609259	372.063813	6.558746
6.040134	368.936295	6.563750
6.358391	366.345824	6.568755
5.914116	374.458741	6.573760
6.055669	371.663066	6.578765
5.596484	378.066674	6.583770
5.872336	370.982141	6.588774
6.114798	378.359446	6.593779
5.837921	371.359846	6.598784
6.184908	362.967423	6.603789
5.982244	374.294765	6.608794
6.220666	369.887818	6.613798
5.991945	370.817902	6.618803
5.667803	369.567778	6.623808
5.985588	357.778437	6.628813
5.969778	382.388288	6.633818
6.259520	372.483456	6.638822
5.984690	370.056014	6.643827
5.790124	367.515369	6.648832
6.121800	366.334049	6.653837
5.915723	369.405264	6.658842
6.150932	368.905713	6.663846
5.968516	356.908891	6.668851
5.683444	361.367727	6.673856
5.724520	362.134343	6.678861
5.521714	371.440844	6.683866
5.774415	372.894449	6.688870
6.119241	378.327104	6.693875
5.676490	378.056205	6.698880
5.844627	378.145960	6.703885
5.982599	371.184251	6.708890
5.951806	378.527987	6.713894
5.843518	374.435434	6.718899
5.788841	371.926326	6.723904
5.719998	376.492877	6.728909
5.515926	378.123684	6.733914
5.599179	370.939078	6.738918
5.876285	382.737341	6.743923
6.340634	384.845771	6.748928
6.416472	372.270359	6.753933
5.744885	384.278977	6.758938
5.936120	372.072408	6.763942
6.101404	372.968356	6.768947
6.166870	365.235799	6.773952
6.071045	367.520462	6.778957
6.023273	370.214300	6.783962
6.018191	366.419603	6.788966
6.065057	376.957997	6.793971
5.929738	372.576609	6.798976
5.985471	371.278405	6.803981
5.811044	384.266988	6.808986
6.053459	382.442384	6.813990
6.067471	378.492894	6.818995
5.869457	382.134883	6.824000
6.010499	373.080473	6.829005
6.110419	375.813537	6.834010
6.077077	370.074171	6.839014
6.404476	368.658263	6.844019
5.875832	374.151411	6.849024
6.386458	364.655610	6.854029
6.236855	377.438630	6.859034
6.196185	382.162421	6.864038
6.241589	364.861797	6.869043
5.846552	362.957267	6.874048
5.963040	351.458689	6.879053
5.657513	351.738302	6.884058
6.334325	366.695449	6.889062
5.997113	351.994114	6.894067
5.627782	349.192011	6.899072
6.079931	357.634070	6.904077
5.848754	358.128599	6.909082
6.013666	373.336980	6.914086
6.112162	363.519993	6.919091
6.100590	360.286240	6.924096
5.895741	344.869094	6.929101
5.707531	345.808858	6.934106
6.150953	361.399759	6.939110
5.794838	356.155915	6.944115
6.122460	360.477881	6.949120
6.423312	359.638268	6.954125
6.084462	349.337544	6.959130
5.753167	334.945224	6.964134
5.831449	341.048082	6.969139
5.762952	347.327523	6.974144
6.016895	336.028906	6.979149
5.954234	342.420046	6.984154
5.934077	329.172608	6.989158
6.075994	337.975408	6.994163
5.755830	345.724675	6.999168
5.899625	343.689269	7.004173
5.932491	366.487331	7.009178
6.239676	361.806895	7.014182
5.959238	349.332310	7.019187
5.973374	344.875027	7.024192
6.307094	336.760849	7.029197
6.012416	341.384739	7.034202
5.848578	334.491669	7.039206
5.878852	345.549443	7.044211
5.455626	335.840991	7.049216
5.587198	347.847863	7.054221
5.834333	368.605837	7.059226
6.000432	364.110611	7.064230
6.187654	371.094329	7.069235
6.165884	367.644329	7.074240
6.018096	368.086799	7.079245
6.182546	372.803622	7.084250
6.198473	357.959472	7.089254
6.216512	349.506978	7.094259
5.844726	341.790362	7.099264
6.215695	338.625691	7.104269
5.641048	344.759208	7.109274
5.792961	332.980231	7.114278
5.805529	340.490515	7.119283
5.806990	352.041597	7.124288
5.888277	358.387053	7.129293
5.816908	371.575635	7.134298
5.857637	377.343661	7.139302
6.010932	370.186942	7.144307
5.974672	363.752834	7.149312
6.088366	362.561170	7.154317
5.914514	379.473978	7.159322
6.035121	366.850131	7.164326
6.072894	371.661190	7.169331
6.088681	375.255019	7.174336
6.242571	359.521968	7.179341
5.631666	360.161433	7.184346
5.826912	361.381938	7.189350
6.152994	367.716637	7.194355
6.125093	373.875433	7.199360
5.929457	352.494697	7.204365
5.458142	357.455095	7.209370
6.015211	361.359220	7.214374
5.770252	363.870773	7.219379
5.804187	372.900095	7.224384
5.788321	366.258890	7.229389
5.970054	371.967602	7.234394
6.005089	373.574579	7.239398
6.251945	369.817367	7.244403
5.584951	387.337122	7.249408
5.810478	375.608889	7.254413
5.791574	378.367511	7.259418
5.770628	372.390998	7.264422
5.865671	379.956138	7.269427
5.974257	379.469818	7.274432
6.024348	371.693036	7.279437
5.947595	382.488342	7.284442
5.901264	376.925937	7.289446
5.633290	375.621346	7.294451
5.846453	378.151506	7.299456
5.988049	374.971164	7.304461
5.887290	382.492108	7.309466
5.982162	370.172128	7.314470
6.243523	377.050268	7.319475
5.837738	372.886916	7.324480
6.049871	374.419836	7.329485
6.020962	378.269072	7.334490
6.079055	375.954423	7.339494
6.132916	376.533158	7.344499
5.941497	384.251795	7.349504
6.132623	380.205061	7.354509
6.076013	383.181136	7.359514
5.909438	374.361359	7.364518
6.192478	378.128163	7.369523
5.595971	388.926202	7.374528
5.982171	371.634954	7.379533
5.980556	381.132654	7.384538
6.217924	380.559445	7.389542
6.212829	370.070463	7.394547
5.951692	380.788113	7.399552
6.056361	374.407069	7.404557
5.801449	382.088350	7.409562
5.646435	376.214200	7.414566
5.984705	379.108836	7.419571
5.899504	380.003363	7.424576
6.129540	378.070212	7.429581
6.294875	380.167285	7.434586
5.987627	383.055543	7.439590
5.910903	376.221260	7.444595
5.629184	385.831549	7.449600
5.880773	374.263963	7.454605
6.204084	373.286960	7.459610
6.057305	378.914609	7.464614
5.985055	373.934513	7.469619
5.799706	380.770755	7.474624
5.952365	387.685806	7.479629
5.999562	380.776090	7.484634
6.220405	378.703677	7.489638
6.166140	380.365862	7.494643
5.998862	384.440014	7.499648
5.881514	381.286680	7.504653
6.254349	374.015641	7.509658
6.168946	383.849596	7.514662
6.547563	376.770769	7.519667
5.935188	367.487094	7.524672
5.808219	357.487863	7.529677
5.931259	349.170835	7.534682
5.872134	350.522364	7.539686
6.041295	347.781817	7.544691
5.890274	354.402436	7.549696
5.900038	338.024933	7.554701
5.897309	351.767254	7.559706
6.034751	358.717462	7.564710
6.282165	352.835810	7.569715
5.700869	351.458004	7.574720
5.658892	352.406257	7.579725
5.629572	367.110537	7.584730
6.005395	364.265098	7.589734
6.495635	372.547954	7.594739
5.650623	376.826943	7.599744
6.217916	371.315653	7.604749
6.022150	380.505273	7.609754
5.835156	373.846077	7.614758
6.118343	369.715368	7.619763
5.732829	374.806419	7.624768
6.094845	365.701880	7.629773
6.148582	380.218023	7.634778
5.744488	364.859534	7.639782
5.955632	363.414893	7.644787
6.062331	375.379332	7.649792
5.911191	375.145677	7.654797
6.081035	379.683537	7.659802
5.795040	373.071680	7.664806
6.125622	372.907977	7.669811
6.095349	379.463960	7.674816
6.102929	354.245078	7.679821
6.176022	352.543761	7.684826
5.503078	354.140769	7.689830
5.642457	353.678760	7.694835
5.998422	377.402895	7.699840
6.120865	372.547684	7.704845
5.879707	379.532747	7.709850
5.648375	383.141668	7.714854
5.973907	381.036169	7.719859
5.918453	377.465652	7.724864
5.850428	383.350505	7.729869
5.958850	377.038294	7.734874
5.930998	383.123784	7.739878
6.336883	382.690046	7.744883
6.265745	384.018307	7.749888
6.107160	379.397674	7.754893
6.003435	365.514072	7.759898
5.842746	355.448692	7.764902
5.892350	352.886936	7.769907
5.913660	371.451435	7.774912
6.310810	373.061905	7.779917
6.027493	365.589430	7.784922
5.701972	359.074875	7.789926
5.893562	361.038269	7.794931
5.848084	357.379390	7.799936
5.954453	376.879399	7.804941
6.483596	372.578901	7.809946
5.862139	369.382897	7.814950
6.043242	363.255596	7.819955
5.570457	359.891973	7.824960
5.485639	359.887189	7.829965
5.937544	377.970818	7.834970
5.770074	383.295858	7.839974
5.971912	372.609401	7.844979
5.795923	383.168154	7.849984
5.798306	380.531721	7.854989
5.932425	383.245520	7.859994
5.790327	384.977962	7.864998
5.701018	378.349580	7.870003
5.771590	378.867741	7.875008
5.840723	374.532475	7.880013
5.824848	375.579116	7.885018
5.998471	378.867173	7.890022
6.030558	386.219857	7.895027
5.779053	383.941573	7.900032
6.060795	372.089119	7.905037
6.336196	381.354875	7.910042
5.675442	380.468185	7.915046
5.870097	377.148257	7.920051
5.529033	379.477298	7.925056
6.185448	381.852519	7.930061
6.331260	378.359432	7.935066
6.237686	376.593216	7.940070
6.296622	374.917420	7.945075
5.887113	383.431058	7.950080
5.893742	382.994243	7.955085
6.301798	372.236513	7.960090
6.145758	375.591283	7.965094
5.827659	391.082735	7.970099
5.685134	386.749691	7.975104
5.766992	385.833603	7.980109
5.753249	381.413672	7.985114
5.994121	376.810585	7.990118
6.155942	376.539294	7.995136
5.730532	379.458636	8.000154
5.848850	375.934661	8.005171
5.805711	379.448266	8.010189
5.847487	373.577605	8.015206
5.984906	377.149933	8.020224
5.857239	386.273257	8.025242
6.055284	369.425382	8.030259
6.122878	378.652819	8.035277
5.820743	384.868106	8.040294
5.990318	371.929510	8.045312
5.768991	388.058642	8.050330
6.057362	392.537619	8.055347
5.843052	386.234869	8.060365
6.251911	412.581787	8.065382
6.570341	394.480098	8.070400
5.654941	383.652669	8.075418
5.895134	379.165842	8.080435
5.994443	385.946736	8.085453
6.253971	404.467345	8.090470
6.171662	386.324337	8.095488
5.918404	386.092375	8.100506
5.814278	384.741121	8.105523
6.273529	399.158723	8.110541
6.068767	403.264474	8.115558
6.240404	397.088447	8.120576
6.036827	395.891295	8.125594
6.216933	398.889076	8.130611
6.184991	378.422008	8.135629
5.620275	392.770001	8.140646
5.784216	404.632245	8.145664
5.894501	406.901272	8.150682
5.762217	409.942416	8.155699
5.984751	414.034432	8.160717
6.430790	407.328706	8.165734
6.419878	414.955113	8.170752
6.341635	407.554407	8.175770
6.566819	412.095790	8.180787
6.465978	406.722994	8.185805
6.440805	405.659315	8.190822
6.053853	386.664876	8.195840
6.052469	380.490880	8.200858
6.212824	391.409421	8.205875
6.255796	388.830472	8.210893
6.179294	381.342501	8.215910
6.073228	378.147376	8.220928
5.938823	393.332427	8.225946
6.102445	409.506110	8.230963
6.522973	407.649044	8.235981
6.232481	408.979499	8.240998
6.420052	400.347717	8.246016
6.246714	393.197920	8.251034
6.214473	384.664665	8.256051
6.006544	380.492985	8.261069
6.193016	400.316528	8.266086
6.171625	407.234578	8.271104
6.127841	410.131793	8.276122
6.146017	423.117021	8.281139
6.529334	404.607634	8.286157
6.263204	414.631229	8.291174
6.481636	410.267943	8.296192
6.337921	413.406528	8.301210
6.221204	417.100179	8.306227
6.589355	410.089970	8.311245
6.033078	400.167936	8.316262
6.247530	400.878344	8.321280
6.260274	409.016968	8.326298
6.608405	417.989450	8.331315
6.701961	397.448675	8.336333
6.212540	394.660725	8.341350
6.103706	390.557391	8.346368
6.557608	381.826008	8.351386
6.256832	385.661068	8.356403
6.494649	385.731727	8.361421
6.134181	385.929107	8.366438
6.167620	383.122748	8.371456
6.327709	395.401477	8.376474
6.110673	406.304756	8.381491
6.508223	409.285498	8.386509
6.194903	421.602730	8.391526
6.567822	413.108287	8.396544
6.607566	419.565843	8.401562
6.570563	411.550475	8.406579
6.216263	398.255812	8.411597
6.178047	400.688523	8.416614
6.187812	405.050688	8.421632
6.471070	412.492386	8.426650
6.312252	409.812262	8.431667
6.603770	406.015714	8.436685
6.419768	414.703774	8.441702
6.584187	407.984563	8.446720
6.786992	404.337489	8.451738
6.245316	413.432025	8.456755
6.603530	402.023217	8.461773
6.452614	405.231086	8.466790
6.564999	396.026424	8.471808
6.437596	386.249420	8.476826
6.195870	399.800107	8.481843
6.373672	395.764830	8.486861
6.261159	405.525878	8.491878
6.300467	416.789470	8.496896
6.753026	417.429630	8.501914
6.512909	413.232361	8.506931
6.735340	409.826282	8.511949
6.506250	415.391849	8.516966
6.369221	409.358049	8.521984
6.751346	413.386985	8.527002
6.393245	416.694141	8.532019
6.687360	408.325004	8.537037
6.534331	426.532208	8.542054
6.471709	404.393365	8.547072
6.444305	410.856011	8.552090
6.421369	410.546919	8.557107
6.445539	405.202470	8.562125
6.302482	407.664219	8.567143
6.407161	417.470663	8.572160
6.305470	402.542461	8.577178
6.494103	413.669783	8.582195
6.672416	405.352455	8.587213
6.552318	413.849087	8.592231
6.526808	420.631337	8.597248
6.664552	410.317001	8.602266
6.490389	411.751434	8.607283
6.666535	411.502531	8.612301
6.461335	414.995102	8.617319
6.434615	417.231469	8.622336
6.675140	415.432687	8.627354
6.484237	416.397841	8.632371
6.513216	411.421218	8.637389
6.688441	414.798961	8.642407
6.698579	416.361859	8.647424
6.684568	406.997212	8.652442
6.352059	418.409144	8.657459
6.933852	413.316265	8.662477
6.213847	423.757715	8.667495
6.480746	438.446167	8.672512
6.907149	429.921719	8.677530
6.671939	450.819429	8.682547
6.875321	449.167204	8.687565
6.873410	440.604010	8.692583
6.565040	447.015685	8.697600
6.744448	435.763245	8.702618
6.656212	446.692206	8.707635
7.009890	445.346865	8.712653
6.898605	432.836739	8.717671
6.489230	423.576880	8.722688
6.644829	428.625627	8.727706
6.692354	441.154640	8.732723
7.146001	430.578187	8.737741
6.747402	435.608508	8.742759
6.756979	433.875346	8.747776
6.851290	425.905283	8.752794
6.866484	423.316453	8.757811
6.637005	412.569405	8.762829
6.541496	433.879148	8.767847
6.705198	433.986952	8.772864
6.974598	432.449186	8.777882
6.623087	443.311736	8.782899
6.605999	445.305326	8.787917
6.675833	447.630837	8.792935
7.040246	446.285198	8.797952
6.899059	434.750674	8.802970
6.793303	443.841775	8.807987
6.565745	438.476035	8.813005
6.691036	448.305760	8.818023
6.817976	446.708286	8.823040
6.991027	434.563483	8.828058
6.614559	440.824140	8.833075
6.596199	443.787913	8.838093
6.829070	441.147755	8.843111
6.767884	442.983510	8.848128
7.138299	439.880065	8.853146
6.894044	443.545990	8.858163
6.801857	447.705377	8.863181
7.110998	435.386441	8.868199
6.904117	445.571095	8.873216
6.994370	437.051222	8.878234
6.829762	438.360285	8.883251
6.894568	434.910580	8.888269
7.056381	439.156012	8.893287
6.651939	442.832863	8.898304
6.919924	438.973083	8.903322
6.779117	444.404411	8.908339
6.583136	447.961987	8.913357
7.021440	449.152223	8.918375
6.937950	454.164424	8.923392
7.307718	445.982328	8.928410
6.420878	462.678513	8.933427
6.762623	467.931205	8.938445
7.135612	467.305650	8.943463
7.121089	471.790819	8.948480
7.167472	475.206498	8.953498
6.949793	477.833708	8.958515
7.101789	480.368631	8.963533
7.068378	472.970619	8.968551
7.321180	477.446151	8.973568
7.243390	464.574927	8.978586
6.889438	449.794252	8.983603
6.985786	444.796152	8.988621
7.196325	458.453114	8.993639
6.850892	446.711440	8.998656
7.198771	453.834275	9.003674
7.104848	474.336108	9.008691
7.030748	455.235070	9.013709
7.458183	458.863305	9.018727
7.107090	454.102302	9.023744
7.033206	442.646886	9.028762
7.074311	449.913607	9.033779
7.139448	447.236615	9.038797
7.212085	448.505782	9.043815
7.009587	451.730747	9.048832
7.090045	446.571822	9.053850
7.083147	455.769893	9.058867
7.434684	466.599129	9.063885
7.324205	455.099467	9.068903
7.214792	457.292530	9.073920
7.445435	446.229310	9.078938
7.205976	450.282256	9.083955
7.241822	442.235841	9.088973
7.137559	442.366674	9.093991
7.230940	453.663967	9.099008
7.084434	444.448332	9.104026
6.649191	443.765837	9.109043
7.190753	450.835407	9.114061
7.534573	451.032514	9.119079
7.197239	455.403443	9.124096
7.310619	442.777358	9.129114
7.361641	443.309603	9.134131
7.237119	445.114397	9.139149
7.673826	436.289093	9.144167
7.294507	442.083096	9.149184
7.255304	440.588851	9.154202
6.982600	450.365577	9.159219
7.064970	449.643002	9.164237
7.267021	447.776476	9.169255
7.356925	446.484371	9.174272
7.228083	445.904062	9.179290
7.348364	442.595844	9.184307
7.086098	433.049224	9.189325
7.383547	440.678018	9.194343
7.296605	456.662401	9.199360
7.487919	454.480786	9.204378
7.339042	448.536706	9.209395
6.819067	448.349313	9.214413
7.225060	467.560998	9.219431
7.401494	477.082155	9.224448
7.559064	471.810893	9.229466
7.765908	468.104979	9.234483
7.702560	458.226320	9.239501
7.586817	438.117338	9.244519
7.102653	455.427730	9.249536
7.193334	437.010160	9.254554
7.521991	435.626149	9.259571
7.102107	446.752310	9.264589
7.825899	452.945093	9.269607
7.401842	455.085452	9.274624
7.613236	436.831162	9.279642
7.272147	448.166106	9.284659
7.066135	445.872830	9.289677
7.485632	452.278269	9.294695
7.655599	470.959201	9.299712
7.363634	463.993704	9.304730
7.900732	469.537273	9.309747
7.361446	448.855298	9.314765
7.545876	441.157380	9.319783
7.417091	457.393115	9.324800
7.478679	441.278981	9.329818
7.318614	444.633320	9.334835
7.360776	463.055108	9.339853
8.012370	465.105678	9.344871
7.488183	454.712358	9.349888
7.717112	451.668309	9.354906
7.274103	454.459400	9.359923
7.343922	451.386244	9.364941
7.454566	449.923521	9.369959
7.259285	461.986091	9.374976
7.258665	460.078270	9.379994
7.510449	468.329260	9.385011
7.172106	479.330082	9.390029
7.500279	475.170643	9.395047
6.817858	471.399039	9.400064
7.109569	471.137236	9.405082
7.319555	475.427462	9.410099
7.987158	499.463837	9.415117
7.937730	482.846657	9.420135
7.905676	479.770256	9.425152
7.685547	480.686515	9.430170
7.632323	473.965653	9.435187
7.149783	472.231155	9.440205
7.284779	471.183610	9.445223
7.761182	483.218738	9.450240
7.564051	481.499656	9.455258
7.560546	485.238380	9.460275
7.816032	510.843946	9.465293
7.618147	501.018982	9.470311
7.842563	503.856639	9.475328
7.697385	499.324431	9.480346
7.785809	484.009194	9.485363
7.495321	490.112778	9.490381
7.634968	489.036517	9.495399
8.060807	496.360223	9.500416
8.037435	500.219630	9.505434
7.698579	488.078397	9.510451
7.455520	485.147572	9.515469
7.796048	479.491617	9.520487
7.553549	477.944173	9.525504
7.621123	490.074325	9.530522
7.919121	499.105523	9.535539
8.026307	506.070858	9.540557
7.957467	485.697916	9.545575
7.970627	476.303938	9.550592
8.046767	484.385876	9.555610
7.881465	473.986667	9.560627
7.483482	483.182667	9.565645
7.798761	479.106641	9.570663
7.927631	482.877905	9.575680
7.702958	485.256127	9.580698
7.883961	469.039175	9.585715
7.515264	474.045378	9.590733
7.534229	486.154727	9.595751
7.993281	499.603761	9.600768
8.042882	494.955032	9.605786
8.060321	490.559600	9.610803
7.655344	481.329682	9.615821
7.994562	492.647583	9.620839
7.746854	496.760358	9.625856
7.862855	502.170521	9.630874
7.779831	498.184915	9.635891
7.767214	496.912602	9.640909
7.832068	498.493134	9.645927
7.932376	505.674522	9.650944
8.091301	502.177757	9.655962
7.899932	503.210302	9.660979
7.255089	512.663510	9.665997
7.518388	506.337181	9.671015
7.785907	502.548216	9.676032
7.699370	505.480068	9.681050
8.147530	504.817192	9.686067
8.030773	509.526213	9.691085
8.110844	510.055530	9.696103
8.167028	508.508219	9.701120
8.058149	496.176937	9.706138
8.273444	500.398098	9.711155
7.899529	506.930548	9.716173
8.010338	496.607420	9.721191
7.784707	505.540550	9.726208
7.999101	504.109879	9.731226
7.938200	502.642438	9.736243
7.960202	505.685460	9.741261
8.085422	495.851582	9.746279
8.163763	506.018857	9.751296
7.576633	506.479635	9.756314
7.822217	503.715048	9.761331
8.128138	513.498727	9.766349
8.082706	509.642114	9.771367
8.302141	513.012474	9.776384
7.525579	517.289409	9.781402
8.116812	528.195391	9.786419
8.188033	531.290508	9.791437
8.080609	526.323597	9.796455
8.275843	536.382912	9.801472
8.278691	534.002754	9.806490
8.476830	531.048800	9.811507
8.105927	523.769026	9.816525
8.264829	500.854018	9.821543
8.047030	505.893845	9.826560
8.243272	515.700374	9.831578
8.070632	505.257386	9.836595
8.207173	521.963900	9.841613
8.319765	530.944278	9.846631
8.315072	521.492212	9.851648
7.975428	520.748944	9.856666
8.382958	512.122374	9.861683
8.040565	523.837038	9.866701
8.442669	533.317492	9.871719
8.725414	525.915228	9.876736
8.123583	514.842223	9.881754
8.337486	496.613820	9.886771
8.227158	503.063542	9.891789
8.241752	509.675163	9.896807
8.029438	497.155898	9.901824
8.058422	515.770735	9.906842
8.251600	514.273603	9.911859
8.359342	523.267768	9.916877
8.410099	528.348537	9.921895
8.324672	524.495282	9.926912
8.387644	528.609171	9.931930
8.381084	531.872819	9.936947
8.261389	527.638396	9.941965
8.423982	534.530625	9.946983
8.508017	537.346910	9.952000
8.243901	536.340324	9.957018
8.951585	536.331168	9.962035
8.320198	509.762487	9.967053
8.124466	516.767359	9.972071
8.342338	514.212229	9.977088
8.325442	526.758551	9.982106
8.574390	516.665284	9.987123
8.257034	514.680890	9.992141
8.620768	529.996110	9.997159
8.546211	517.647133	10.002176
8.352329	511.323833	10.007194
8.357143	510.748789	10.012211
8.469370	520.601876	10.017229
8.368390	516.394771	10.022247
8.501631	531.084343	10.027264
8.574198	534.693306	10.032282
8.497842	529.215458	10.037299
8.535654	530.308042	10.042317
8.563753	531.767709	10.047335
8.837264	525.280170	10.052352
8.031816	512.725577	10.057370
8.275502	525.593423	10.062387
8.431471	537.420382	10.067405
8.299088	531.361067	10.072423
8.739146	530.856584	10.077440
8.645022	538.586057	10.082458
8.746875	536.092510	10.087475
8.808080	542.246141	10.092493
8.352863	534.188429	10.097511
9.061336	536.173026	10.102528
8.464335	530.536290	10.107546
8.257858	509.491125	10.112563
8.555771	525.031741	10.117581
8.320817	527.359514	10.122599
8.542438	523.270317	10.127616
8.368479	541.616030	10.132634
8.548305	529.414729	10.137651
8.563301	529.677594	10.142669
8.645261	542.334534	10.147687
8.541701	531.830810	10.152704
8.463066	543.520006	10.157722
8.557990	528.881465	10.162739
8.542358	526.754803	10.167757
8.415414	533.822119	10.172775
8.475268	535.962224	10.177792
8.518163	537.646959	10.182810
8.560579	556.960368	10.187827
8.780705	562.471726	10.192845
8.678000	562.473490	10.197863
9.087019	556.695285	10.202880
8.619317	548.099287	10.207898
8.849544	549.787899	10.212915
9.251534	543.499154	10.217933
8.762630	545.020941	10.222951
9.198686	533.997416	10.227968
8.515229	530.829683	10.232986
8.483892	537.509622	10.238003
8.658866	535.210642	10.243021
8.444422	543.458227	10.248039
9.008340	538.349171	10.253056
8.541416	558.234058	10.258074
8.913957	564.671118	10.263091
9.168669	560.516121	10.268109
8.602926	552.805733	10.273127
9.173425	564.835510	10.278144
8.929236	547.986917	10.283162
8.841997	541.775973	10.288179
8.710472	541.751896	10.293197
8.975572	552.155409	10.298215
9.180968	558.299879	10.303232
9.118743	545.123813	10.308250
8.845866	548.460801	10.313267
8.786214	543.825684	10.318285
8.453914	532.592497	10.323303
8.969169	549.230451	10.328320
9.131666	561.052906	10.333338
8.581831	560.494538	10.338355
9.281080	562.742814	10.343373
9.129797	562.037888	10.348391
8.986800	559.940340	10.353408
9.060805	563.920159	10.358426
8.679328	553.526017	10.363443
8.861875	568.456736	10.368461
8.725369	563.222627	10.373479
8.986225	562.195115	10.378496
8.996897	572.837697	10.383514
8.736875	567.221620	10.388531
9.068011	566.868180	10.393549
8.949665	569.838563	10.398567
8.868442	564.399589	10.403584
9.267525	564.747670	10.408602
9.113631	555.878198	10.413619
9.120114	561.067947	10.418637
9.110025	558.515451	10.423655
9.329410	552.393959	10.428672
9.014581	565.715976	10.433690
9.232507	564.994513	10.438707
9.368466	562.809435	10.443725
8.924199	565.268341	10.448743
9.177978	565.397078	10.453760
9.304530	571.725021	10.458778
9.139098	569.175268	10.463795
9.093788	565.454223	10.468813
8.959525	569.258760	10.473831
9.060821	563.462918	10.478848
9.004873	569.160917	10.483866
9.216989	568.950055	10.488883
9.337651	552.949048	10.493901
9.091177	566.351779	10.498919
8.797075	567.721910	10.503936
8.914634	566.308122	10.508954
8.941817	566.284090	10.513971
9.079202	564.170711	10.518989
8.834260	585.139390	10.524007
9.399213	591.539743	10.529024
9.224174	593.980237	10.534042
9.213166	599.518588	10.539059
9.485407	592.723812	10.544077
9.688418	605.354009	10.549095
9.161426	587.084194	10.554112
9.460464	582.424919	10.559130
9.183851	581.535135	10.564147
9.475457	582.713413	10.569165
9.413370	588.146937	10.574183
9.512003	563.741803	10.579200
9.447391	567.258999	10.584218
9.605498	573.933723	10.589235
9.317914	571.169657	10.594253
9.253951	565.730290	10.599271
9.270855	569.162868	10.604288
9.198814	568.627585	10.609306
9.222158	566.128114	10.614323
9.455598	591.654011	10.619341
9.323071	597.292447	10.624359
9.486306	599.705871	10.629376
9.552065	600.553142	10.634394
9.153930	594.027685	10.639411
9.703530	598.497403	10.644429
9.601122	608.890838	10.649447
9.574799	604.465900	10.654464
9.437465	590.598214	10.659482
9.731558	585.777780	10.664499
9.576136	571.251029	10.669517
9.394465	577.997850	10.674535
9.623418	573.964012	10.679552
9.516346	558.256784	10.684570
9.235877	574.053139	10.689587
9.478434	584.170301	10.694605
9.595393	588.129840	10.699623
9.857257	601.842706	10.704640
9.582823	568.309328	10.709658
9.323315	575.308726	10.714675
9.948597	583.110632	10.719693
9.769761	575.037729	10.724711
9.325341	564.331115	10.729728
9.324444	568.582611	10.734746
9.431739	580.487810	10.739763
9.505184	595.522395	10.744781
9.483374	599.886685	10.749799
9.530514	602.155745	10.754816
9.771269	599.694832	10.759834
9.525828	608.981029	10.764851
9.728909	594.075684	10.769869
9.836966	600.680066	10.774887
9.627046	605.260053	10.779904
10.079986	591.939865	10.784922
9.674567	605.060297	10.789939
9.521040	595.317589	10.794957
9.538020	601.822381	10.799975
9.447007	608.984954	10.804992
9.590393	598.417051	10.810010
9.085572	613.529998	10.815027
9.401315	602.695566	10.820045
9.527558	590.355660	10.825063
9.670249	606.354896	10.830080
9.679445	613.812462	10.835098
9.525480	620.678221	10.840115
9.793453	613.973100	10.845133
9.374972	633.809733	10.850151
9.585615	624.669586	10.855168
9.620879	623.564610	10.860186
9.728067	631.484734	10.865203
9.767127	618.568583	10.870221
9.697949	617.842902	10.875239
9.788727	625.432829	10.880256
9.615767	622.807947	10.885274
9.543827	628.816129	10.890291
9.766046	631.796960	10.895309
9.915146	647.974278	10.900327
9.816431	654.366250	10.905344
10.186121	658.110551	10.910362
9.998459	660.221022	10.915379
10.223085	633.402807	10.920397
9.797743	622.173221	10.925415
9.624130	630.425224	10.930432
10.151683	640.554269	10.935450
10.292118	644.026772	10.940467
10.722519	631.371069	10.945485
10.181380	632.299745	10.950503
9.845478	630.985099	10.955520
10.120681	618.748383	10.960538
9.993603	619.318924	10.965555
10.330246	629.123874	10.970573
10.504221	628.022937	10.975591
10.134281	633.629278	10.980608
10.553315	624.164297	10.985626
10.289460	628.498038	10.990643
10.034836	626.501195	10.995661
10.402625	622.601357	11.000679
10.167793	621.871268	11.005696
10.343520	595.153702	11.010714
9.638656	616.759048	11.015731
10.116839	612.711171	11.020749
10.000002	605.739596	11.025767
9.877974	621.940733	11.030784
10.434280	618.484943	11.035802
10.335175	625.467991	11.040819
10.115900	626.680219	11.045837
10.188643	620.455105	11.050855
10.230396	613.664560	11.055872
10.214122	626.863683	11.060890
9.844650	626.659681	11.065907
10.183881	623.293493	11.070925
10.073257	630.826271	11.075943
10.088258	628.848833	11.080960
9.990255	617.260489	11.085978
9.983828	625.424931	11.090995
10.139659	620.560518	11.096013
10.298727	624.504153	11.101031
10.354961	635.638855	11.106048
10.648786	628.675273	11.111066
10.275914	631.707707	11.116083
10.045405	625.702457	11.121101
10.268299	629.256093	11.126119
9.998539	626.273168	11.131136
10.456280	622.263208	11.136154
10.185456	623.125169	11.141171
10.163662	629.378951	11.146189
10.423291	625.429677	11.151207
10.290423	635.093467	11.156224
10.560893	619.185524	11.161242
10.042439	631.349360	11.166259
10.082533	632.493829	11.171277
10.156967	634.868598	11.176295
10.289736	655.697900	11.181312
10.491771	657.050011	11.186330
10.466908	657.746546	11.191347
10.880119	674.327106	11.196365
11.098255	647.777308	11.201383
10.423413	646.215880	11.206400
10.385745	628.681818	11.211418
10.351134	621.185331	11.216435
10.593060	632.260313	11.221453
10.458129	628.784726	11.226471
10.244814	623.836563	11.231488
10.291406	623.108085	11.236506
10.477920	650.210026	11.241523
10.434111	653.780978	11.246541
10.855397	656.850053	11.251559
10.319906	656.555498	11.256576
10.747823	652.448314	11.261594
10.524564	655.550988	11.266611
10.717431	653.890443	11.271629
10.913524	652.446546	11.276647
10.240743	641.383993	11.281664
10.528536	650.257747	11.286682
10.463157	650.470720	11.291699
10.705285	651.035453	11.296717
10.651707	653.141477	11.301735
10.477371	661.210975	11.306752
10.711543	660.434766	11.311770
10.562543	655.311921	11.316787
10.640200	656.949889	11.321805
10.743746	658.590073	11.326823
10.519558	660.229213	11.331840
10.609817	663.821506	11.336858
10.555518	662.557052	11.341875
10.741718	651.543443	11.346893
10.689377	659.431393	11.351911
10.301656	651.794172	11.356928
10.461941	655.488943	11.361946
10.222724	662.040232	11.366963
10.401310	675.639393	11.371981
10.741507	683.886516	11.376999
10.631406	703.065896	11.382016
10.849785	684.757610	11.387034
11.184790	698.003543	11.392051
10.756811	698.101082	11.397069
10.941256	687.196377	11.402087
10.598027	694.747454	11.407104
10.850710	687.612038	11.412122
11.021197	688.606837	11.417139
11.097105	696.721399	11.422157
11.266082	687.886960	11.427175
11.032671	700.308704	11.432192
11.001018	677.488594	11.437210
10.942274	673.070667	11.442227
11.133534	677.993450	11.447245
10.971679	662.687218	11.452263
10.927240	666.254242	11.457280
10.879185	668.924107	11.462298
10.843048	657.362017	11.467315
10.760092	665.710256	11.472333
11.074993	674.014201	11.477351
11.042590	685.498856	11.482368
10.972645	686.889619	11.487386
10.936383	677.749013	11.492403
10.960108	683.284507	11.497421
10.756093	688.802533	11.502439
10.735892	691.685277	11.507456
10.974236	687.777588	11.512474
10.953664	696.962023	11.517491
10.829746	698.166469	11.522509
10.912351	686.567808	11.527527
10.766169	697.904871	11.532544
10.994351	684.836370	11.537562
10.769787	683.856105	11.542579
10.744104	700.146500	11.547597
11.150668	702.560763	11.552615
11.229656	720.999802	11.557632
11.308817	724.185852	11.562650
11.451935	725.827081	11.567667
10.941963	716.206971	11.572685
11.384072	710.690315	11.577703
11.337039	715.637434	11.582720
11.753944	711.953331	11.587738
11.344863	691.070116	11.592755
11.101782	697.095389	11.597773
11.471055	693.820659	11.602791
10.950253	693.593348	11.607808
10.657874	694.899635	11.612826
11.207900	710.211999	11.617843
10.944211	723.542331	11.622861
11.876661	715.317290	11.627879
11.396576	726.747147	11.632896
11.242990	726.977257	11.637914
11.505238	720.658001	11.642931
11.443183	719.981621	11.647949
11.187274	698.242337	11.652967
11.201651	707.096852	11.657984
11.139336	711.598649	11.663002
11.599858	718.050461	11.668019
11.776155	715.027753	11.673037
11.473921	714.043494	11.678055
11.407638	703.507513	11.683072
11.224767	702.820594	11.688090
11.615173	716.960560	11.693107
11.504821	722.806360	11.698125
11.589640	712.955501	11.703143
11.166852	699.764396	11.708160
11.448935	706.447523	11.713178
11.481597	719.810160	11.718195
11.396489	732.055089	11.723213
11.764125	715.315396	11.728231
11.688932	727.847210	11.733248
11.691088	717.585779	11.738266
11.542898	704.538033	11.743283
11.080446	715.405233	11.748301
11.465272	719.181884	11.753319
11.571226	723.872566	11.758336
11.660821	731.660734	11.763354
11.960186	729.701237	11.768371
11.592152	721.891960	11.773389
12.000524	730.817965	11.778407
11.235265	698.491481	11.783424
11.451172	714.865761	11.788442
11.536670	720.570554	11.793459
11.358513	728.687658	11.798477
11.478667	725.256689	11.803495
11.485171	736.473388	11.808512
11.655533	729.046989	11.813530
11.551853	732.118699	11.818547
11.424263	731.869900	11.823565
11.731604	726.435637	11.828583
11.739289	742.241225	11.833600
11.333834	727.982572	11.838618
11.636298	724.197028	11.843635
11.702319	725.924508	11.848653
11.648191	720.253584	11.853671
11.495031	728.768351	11.858688
11.879532	742.606815	11.863706
11.796081	750.429298	11.868723
11.829983	768.928493	11.873741
11.653141	754.961302	11.878759
12.065283	754.349046	11.883776
12.090433	762.826885	11.888794
11.888599	745.902978	11.893811
11.687570	741.472627	11.898829
12.114938	746.175836	11.903847
12.070771	750.925778	11.908864
11.604234	738.320795	11.913882
12.041275	743.993282	11.918899
12.042815	759.861506	11.923917
11.759004	753.287172	11.928935
12.227524	756.554524	11.933952
11.883394	745.374110	11.938970
11.943905	748.115991	11.943987
11.874908	754.129049	11.949005
11.755650	756.245745	11.954023
12.097164	753.252112	11.959040
11.610288	759.662812	11.964058
12.125509	754.680116	11.969075
12.122888	751.018592	11.974093
12.164938	746.649820	11.979111
12.491357	756.004265	11.984128
12.224256	757.916894	11.989146
12.190844	752.432460	11.994163
11.965903	743.728627	11.999181
12.157542	743.612468	12.004199
12.321166	740.975142	12.009216
12.375017	737.861860	12.014234
12.093044	725.630737	12.019251
12.026786	721.116026	12.024269
11.930388	724.315541	12.029287
12.177528	741.208406	12.034304
12.261610	744.912052	12.039322
12.291559	741.974635	12.044339
12.450368	753.330023	12.049357
11.972384	738.293143	12.054375
12.285523	740.341625	12.059392
12.299839	758.220344	12.064410
12.226646	746.989840	12.069427
12.206489	754.909718	12.074445
12.080135	756.932624	12.079463
12.300731	746.750112	12.084480
12.241257	754.600518	12.089498
12.094791	752.013846	12.094515
12.009305	749.205522	12.099533
12.196380	757.280685	12.104551
12.165241	743.885277	12.109568
11.937573	757.172980	12.114586
12.064727	744.413097	12.119603
12.059465	752.407467	12.124621
11.927229	758.241447	12.129639
12.256654	770.057830	12.134656
12.263053	779.838630	12.139674
12.591285	784.532451	12.144691
12.094013	779.903653	12.149709
12.143652	776.473992	12.154727
12.629876	771.096158	12.159744
12.293025	777.908763	12.164762
12.401810	780.224738	12.169779
12.366784	774.632315	12.174797
12.586289	776.627195	12.179815
12.455696	777.100408	12.184832
12.425964	778.477449	12.189850
12.397310	780.454198	12.194867
12.240049	781.147722	12.199885
12.158548	787.608150	12.204903
12.520950	775.613544	12.209920
12.545871	786.352916	12.214938
12.726779	793.566583	12.219955
12.616887	801.584469	12.224973
12.448175	806.870170	12.229991
12.715705	805.946244	12.235008
12.560750	809.523988	12.240026
12.747216	802.257461	12.245043
12.856975	807.882306	12.250061
12.688740	807.661183	12.255079
13.031384	799.451007	12.260096
12.656544	797.165602	12.265114
12.770342	791.246863	12.270131
12.842927	781.755296	12.275149
12.997875	785.566510	12.280167
12.941801	774.550536	12.285184
12.369566	786.545660	12.290202
12.494216	783.957969	12.295219
12.885021	794.308989	12.300237
12.784686	804.110887	12.305255
12.796463	784.693434	12.310272
12.485489	796.630431	12.315290
13.056162	809.053016	12.320307
12.768988	816.182268	12.325325
12.862572	817.928131	12.330343
13.173693	815.701671	12.335360
12.779599	812.607786	12.340378
13.142845	808.265133	12.345395
13.282373	803.867639	12.350413
12.763909	783.185510	12.355431
12.703146	777.041539	12.360448
12.781586	792.165533	12.365466
12.859413	803.434163	12.370483
13.157698	804.071102	12.375501
12.790418	815.525188	12.380519
12.953181	807.178133	12.385536
12.418512	807.542371	12.390554
13.095488	810.070988	12.395571
12.799564	808.772353	12.400589
12.649158	810.879934	12.405607
12.705985	803.894527	12.410624
12.691008	811.618241	12.415642
12.790025	813.744336	12.420659
13.279910	821.639101	12.425677
13.172798	837.243425	12.430695
13.268213	818.675628	12.435712
12.928598	817.555539	12.440730
13.022403	815.138854	12.445747
12.858486	823.046410	12.450765
13.246639	840.287369	12.455783
13.465435	837.618374	12.460800
13.380762	848.245905	12.465818
13.079180	843.079919	12.470835
13.282271	831.036315	12.475853
13.048773	823.494955	12.480871
13.279614	832.555064	12.485888
13.317802	838.821159	12.490906
13.172524	842.725597	12.495923
13.335365	839.682455	12.500941
13.569810	843.918752	12.505959
13.995540	842.180439	12.510976
13.569946	826.853862	12.515994
13.417283	819.303868	12.521011
13.414310	812.985205	12.526029
13.254668	826.854628	12.531047
13.069552	814.576922	12.536064
13.325954	825.411506	12.541082
13.298915	819.837329	12.546099
13.746331	815.538037	12.551117
13.274016	823.162075	12.556135
13.475741	813.507834	12.561152
13.260382	824.090128	12.566170
13.283314	829.232375	12.571187
13.416046	816.313962	12.576205
13.562635	817.801899	12.581223
13.792440	815.993822	12.586240
13.232354	813.722003	12.591258
13.562432	816.261601	12.596275
13.680278	809.312948	12.601293
13.323964	815.314273	12.606311
13.199105	808.373945	12.611328
13.219541	826.227818	12.616346
13.420009	846.544710	12.621363
13.407013	839.785451	12.626381
13.630286	842.452821	12.631399
13.857429	845.316169	12.636416
13.490704	856.566098	12.641434
13.337513	857.788876	12.646451
13.558310	851.130024	12.651469
13.385560	854.241809	12.656487
13.700011	844.099322	12.661504
13.610641	849.725699	12.666522
13.348729	854.617741	12.671539
13.665053	840.999207	12.676557
13.164708	863.346742	12.681575
13.397728	848.055073	12.686592
13.361466	866.980668	12.691610
13.579461	878.281100	12.696627
13.865271	875.497204	12.701645
13.977402	874.337290	12.706663
13.836864	890.515199	12.711680
14.078927	883.848587	12.716698
13.880560	886.544020	12.721715
14.268545	888.734751	12.726733
14.296905	879.114729	12.731751
14.223578	859.794597	12.736768
13.896388	863.606684	12.741786
13.319081	845.965628	12.746803
13.650599	850.149671	12.751821
13.438749	875.826583	12.756839
13.717898	867.505725	12.761856
13.934066	877.429446	12.766874
13.872277	885.596976	12.771891
14.009639	875.869884	12.776909
13.899862	884.031173	12.781927
14.172899	877.317524	12.786944
14.013898	873.628380	12.791962
13.709189	881.490742	12.796979
14.180363	866.233798	12.801997
13.492195	881.813743	12.807015
13.810509	887.188344	12.812032
13.882571	881.997105	12.817050
13.234813	892.963249	12.822067
13.882137	903.428516	12.827085
13.989783	910.021487	12.832103
14.248821	918.938626	12.837120
14.642730	915.502523	12.842138
14.301625	916.954553	12.847155
14.351672	907.006185	12.852173
14.601088	896.855812	12.857191
13.879645	894.599626	12.862208
14.091379	887.003549	12.867226
13.881459	894.764737	12.872243
14.213811	903.427078	12.877261
14.329262	909.517766	12.882279
14.147840	911.255948	12.887296
14.413267	911.927549	12.892314
14.407128	916.466275	12.897331
14.447048	913.889415	12.902349
14.285805	914.872528	12.907367
14.171989	917.351864	12.912384
14.304989	913.756849	12.917402
14.128102	912.929389	12.922419
14.147190	912.095128	12.927437
14.285757	920.954238	12.932455
14.193672	917.298997	12.937472
14.587310	920.332643	12.942490
14.657143	921.708298	12.947507
14.425209	921.202969	12.952525
14.307918	921.134026	12.957543
14.306989	924.795082	12.962560
14.391228	927.944417	12.967578
14.402365	930.547272	12.972595
14.655594	920.040313	12.977613
14.288686	917.212436	12.982631
14.634271	921.614803	12.987648
14.607913	918.835449	12.992666
14.433698	921.134053	12.997683
14.420545	917.962430	13.002701
14.542107	921.969122	13.007719
14.425003	917.630442	13.012736
14.555099	921.943443	13.017754
14.512261	927.708885	13.022771
14.363529	915.476946	13.027789
14.524769	934.314876	13.032807
14.666081	937.739868	13.037824
14.992637	940.995000	13.042842
14.829915	952.510739	13.047859
14.870695	933.641258	13.052877
14.789222	925.068703	13.057895
14.432692	921.665787	13.062912
14.606066	934.876738	13.067930
14.439584	946.827761	13.072947
15.017372	944.652866	13.077965
14.793661	948.271625	13.082983
15.001285	948.339601	13.088000
14.858973	953.648741	13.093018
14.493383	957.435018	13.098035
14.878845	952.127997	13.103053
15.044241	947.926448	13.108071
14.476129	956.373423	13.113088
14.772910	953.074307	13.118106
15.024121	955.991858	13.123123
14.892731	952.566096	13.128141
14.789360	952.134975	13.133159
14.820436	952.911928	13.138176
15.052232	954.947608	13.143194
14.876519	956.326155	13.148211
14.981353	946.769523	13.153229
14.703385	956.052545	13.158247
14.360797	944.601307	13.163264
14.634753	952.443454	13.168282
15.014741	971.058698	13.173299
15.181327	971.272310	13.178317
15.037922	965.640160	13.183335
15.242144	966.397652	13.188352
15.191807	959.764372	13.193370
14.803205	974.018259	13.198387
14.999473	978.695078	13.203405
15.186225	983.596267	13.208423
15.072957	977.271555	13.213440
15.161661	984.340145	13.218458
15.034043	998.481743	13.223475
15.103210	983.324874	13.228493
15.204082	991.890897	13.233511
15.364729	977.503129	13.238528
15.322323	986.760625	13.243546
15.431225	990.335939	13.248563
15.498740	987.889031	13.253581
15.792538	984.167738	13.258599
15.175048	973.023477	13.263616
15.505164	946.487035	13.268634
15.305054	953.097131	13.273651
15.310461	954.972719	13.278669
15.276915	949.050322	13.283687
15.095453	960.575463	13.288704
15.348590	964.083635	13.293722
14.962662	982.736016	13.298739
15.273203	976.609625	13.303757
15.422729	982.579869	13.308775
15.427382	976.189714	13.313792
15.768844	964.675306	13.318810
15.521186	983.367425	13.323827
15.450822	983.317788	13.328845
15.444969	985.827906	13.333863
15.263905	977.294611	13.338880
15.449373	972.023685	13.343898
15.453596	979.042170	13.348915
15.388226	980.833707	13.353933
15.756128	989.538147	13.358951
15.339028	975.366508	13.363968
15.600838	986.304920	13.368986
15.599437	989.247494	13.374003
15.510810	980.669792	13.379021
15.788707	983.658712	13.384039
15.491577	989.282080	13.389056
15.522607	983.910513	13.394074
15.293440	990.691736	13.399091
15.527019	1008.045914	13.404109
15.978946	1009.359022	13.409127
15.668184	1023.038475	13.414144
15.669199	1016.579428	13.419162
15.330011	1017.038015	13.424179
15.527750	1015.818479	13.429197
15.630746	1014.468563	13.434215
15.417017	1026.403641	13.439232
15.720404	1020.433801	13.444250
15.631033	1024.942227	13.449267
15.822577	1013.973432	13.454285
16.022595	1007.707447	13.459303
16.189713	1025.296801	13.464320
16.230272	1012.503082	13.469338
15.978500	1026.105577	13.474355
15.927226	1019.615118	13.479373
15.871072	1022.912455	13.484391
15.955605	1027.053126	13.489408
16.128237	1016.672984	13.494426
15.812935	1013.947564	13.499443
16.046691	1009.347170	13.504461
16.232652	1028.048279	13.509479
15.850573	1016.147981	13.514496
15.806481	1007.228611	13.519514
16.034994	1023.170503	13.524531
15.841658	1012.179307	13.529549
16.092788	1021.281245	13.534567
15.931901	1017.896754	13.539584
15.895500	1007.370781	13.544602
15.934830	1025.142840	13.549619
16.225274	1043.248650	13.554637
16.447271	1042.114458	13.559655
16.350721	1030.072196	13.564672
15.991943	1025.445233	13.569690
16.243849	1028.427435	13.574707
16.250017	1031.064291	13.579725
16.444924	1039.399189	13.584743
16.057579	1031.172643	13.589760
16.043977	1032.827307	13.594778
16.555990	1039.103255	13.599795
16.065289	1044.433984	13.604813
16.345416	1034.637537	13.609831
16.092399	1048.689490	13.614848
16.171256	1046.759999	13.619866
16.439326	1041.676545	13.624883
16.277443	1044.106374	13.629901
16.327429	1039.195257	13.634919
16.057896	1051.481053	13.639936
16.089201	1046.490063	13.644954
16.191471	1049.271447	13.649971
16.012055	1046.530650	13.654989
16.476934	1055.171963	13.660007
16.276506	1077.730533	13.665024
16.291063	1074.035981	13.670042
16.453487	1087.095257	13.675059
16.402203	1078.070163	13.680077
16.621230	1092.598186	13.685095
16.504204	1091.485968	13.690112
16.781055	1082.348780	13.695130
16.984651	1077.520613	13.700147
16.835536	1089.466416	13.705165
16.529241	1081.704321	13.710183
16.799291	1078.248206	13.715200
16.811393	1089.913079	13.720218
16.820395	1080.122243	13.725235
16.819329	1082.077939	13.730253
16.644551	1074.384255	13.735271
16.771500	1080.437586	13.740288
16.718241	1071.533471	13.745306
16.663281	1071.904642	13.750323
16.876164	1084.738095	13.755341
17.006489	1073.078706	13.760359
16.696214	1074.216948	13.765376
16.836011	1075.793912	13.770394
16.537033	1076.879705	13.775411
16.793660	1078.929602	13.780429
16.807628	1075.967109	13.785447
16.692971	1082.747063	13.790464
16.449866	1077.317046	13.795482
16.553436	1074.778648	13.800499
16.596523	1083.033067	13.805517
16.738763	1077.878482	13.810535
16.781192	1086.650247	13.815552
17.109268	1091.115685	13.820570
16.966655	1102.619553	13.825587
17.062329	1113.322169	13.830605
17.180072	1101.430232	13.835623
17.002907	1097.511299	13.840640
16.887516	1101.258428	13.845658
17.183484	1111.475459	13.850675
16.981585	1117.921873	13.855693
17.310239	1110.350058	13.860711
17.095553	1121.658995	13.865728
17.348922	1109.192566	13.870746
17.408405	1107.434547	13.875763
17.033997	1097.622431	13.880781
17.525089	1073.408478	13.885799
17.044578	1084.344461	13.890816
16.981467	1081.277796	13.895834
17.121884	1089.570652	13.900851
17.301912	1108.013335	13.905869
17.474160	1103.001593	13.910887
17.106164	1112.656417	13.915904
17.168844	1113.868240	13.920922
17.285069	1106.031780	13.925939
16.853344	1110.028203	13.930957
17.368294	1104.521513	13.935975
17.270849	1105.157143	13.940992
17.078155	1112.965191	13.946010
17.263405	1107.229372	13.951027
16.940590	1114.132505	13.956045
17.072213	1103.694920	13.961063
17.102789	1119.741855	13.966080
17.461484	1125.338077	13.971098
17.779424	1131.608248	13.976115
17.543099	1134.719574	13.981133
17.679934	1134.885654	13.986151
17.870780	1136.458715	13.991168
17.377955	1119.646254	13.996186
17.727507	1119.960220	14.001203
17.543231	1124.741994	14.006221
17.598320	1125.813757	14.011239
17.536304	1126.827721	14.016256
17.505474	1129.389029	14.021274
17.822992	1123.541794	14.026291
17.711381	1130.331697	14.031309
17.842847	1137.993289	14.036327
17.683869	1136.178275	14.041344
17.581831	1132.291005	14.046362
18.009370	1131.175586	14.051379
17.733200	1131.029076	14.056397
17.860775	1135.497745	14.061415
17.685717	1144.490888	14.066432
17.883004	1135.029274	14.071450
17.719504	1132.730640	14.076467
17.492869	1137.425338	14.081485
17.884824	1130.901735	14.086503
17.567607	1132.509554	14.091520
17.565341	1132.775774	14.096538
17.670088	1130.847701	14.101555
17.793281	1128.401312	14.106573
17.978823	1126.689377	14.111591
17.853269	1133.074763	14.116608
17.514008	1136.986042	14.121626
17.933043	1143.811070	14.126643
17.867336	1154.723623	14.131661
18.032900	1153.940228	14.136679
17.759722	1168.715386	14.141696
18.007569	1161.266724	14.146714
17.927020	1155.278603	14.151731
17.924040	1170.818229	14.156749
18.048001	1165.932340	14.161767
18.150266	1171.912043	14.166784
17.991707	1171.056643	14.171802
18.253902	1160.846218	14.176819
18.205670	1167.287727	14.181837
17.757374	1174.700323	14.186855
18.350749	1164.873086	14.191872
17.959042	1164.365614	14.196890
18.170573	1167.608018	14.201907
17.874638	1175.402062	14.206925
18.497062	1179.608483	14.211943
18.194378	1166.051219	14.216960
18.243913	1164.854589	14.221978
18.460971	1176.787576	14.226995
18.267958	1190.180241	14.232013
18.720888	1182.171582	14.237031
18.431499	1171.115056	14.242048
18.387612	1171.291911	14.247066
18.435554	1157.678285	14.252083
18.426349	1165.108455	14.257101
18.431438	1174.163954	14.262119
18.438108	1173.649101	14.267136
18.277722	1186.086329	14.272154
18.974444	1190.945327	14.277171
18.710397	1185.505348	14.282189
18.661666	1172.769158	14.287207
18.493430	1172.221803	14.292224
18.489279	1170.241064	14.297242
18.468061	1170.996361	14.302259
19.057966	1183.650876	14.307277
18.799396	1170.709839	14.312295
18.968123	1167.367086	14.317312
18.587523	1162.945820	14.322330
18.757014	1160.836402	14.327347
18.682192	1167.220308	14.332365
18.825331	1154.805910	14.337383
18.788177	1161.844109	14.342400
18.650203	1158.662460	14.347418
18.731647	1158.874498	14.352435
18.664211	1165.389444	14.357453
18.281171	1167.855250	14.362471
18.990934	1187.719884	14.367488
18.848432	1193.152345	14.372506
18.991079	1199.345035	14.377523
18.838310	1193.701653	14.382541
18.828002	1195.946049	14.387559
18.955545	1197.434121	14.392576
18.819421	1190.811180	14.397594
18.560621	1198.791194	14.402611
18.602472	1192.491931	14.407629
18.425374	1198.834100	14.412647
18.588932	1193.754288	14.417664
18.958493	1200.912269	14.422682
19.309255	1219.651030	14.427699
18.996267	1215.006405	14.432717
19.066177	1222.964583	14.437735
19.468377	1219.740888	14.442752
18.896428	1213.250778	14.447770
19.658779	1217.069380	14.452787
19.018047	1204.281023	14.457805
19.298638	1191.077666	14.462823
19.096759	1200.679506	14.467840
18.696826	1203.065249	14.472858
19.158498	1220.563242	14.477875
19.278639	1236.614982	14.482893
19.233713	1226.246444	14.487911
19.348562	1235.647366	14.492928
18.864562	1226.186887	14.497946
19.110860	1222.044815	14.502963
19.512166	1229.585296	14.507981
19.342301	1225.285853	14.512999
19.613981	1214.103509	14.518016
19.146520	1231.890672	14.523034
19.375417	1218.232916	14.528051
19.586889	1214.552434	14.533069
19.221216	1227.219258	14.538087
19.632387	1222.044785	14.543104
19.279166	1227.168633	14.548122
19.226485	1219.141363	14.553139
19.673241	1216.344684	14.558157
19.344356	1226.694972	14.563175
19.615857	1228.062421	14.568192
19.479959	1228.910480	14.573210
19.455872	1230.663143	14.578227
19.738070	1223.158586	14.583245
19.300627	1225.604066	14.588263
19.517490	1239.429745	14.593280
19.912860	1249.585960	14.598298
19.878979	1256.768717	14.603315
19.843660	1247.472228	14.608333
19.787265	1231.516900	14.613351
20.108680	1224.715788	14.618368
19.663811	1233.784668	14.623386
19.335518	1222.826843	14.628403
20.011772	1232.391833	14.633421
19.675819	1261.265572	14.638439
20.027038	1246.142135	14.643456
20.108354	1256.116827	14.648474
19.867025	1242.884933	14.653491
19.882289	1229.985389	14.658509
20.082200	1249.084496	14.663527
20.338949	1226.718193	14.668544
19.783493	1230.635307	14.673562
19.826821	1228.159587	14.678579
20.077084	1225.028903	14.683597
19.873887	1218.127316	14.688615
19.893854	1239.246972	14.693632
19.799730	1246.329068	14.698650
19.570967	1258.071466	14.703667
19.839908	1250.879864	14.708685
19.980889	1250.826200	14.713703
19.659757	1258.838196	14.718720
19.594494	1256.319207	14.723738
20.065510	1274.335517	14.728755
20.179989	1279.352763	14.733773
20.053483	1281.119011	14.738791
20.523391	1282.317084	14.743808
20.562223	1277.564502	14.748826
20.338835	1279.884669	14.753843
20.707103	1276.090085	14.758861
20.184510	1258.440397	14.763879
20.474208	1254.245875	14.768896
20.183666	1246.208105	14.773914
20.066524	1255.474766	14.778931
20.337985	1268.546094	14.783949
20.004628	1275.305394	14.788967
20.644879	1281.056884	14.793984
20.515367	1286.898978	14.799002
20.284472	1279.226865	14.804019
20.492382	1286.206318	14.809037
20.184038	1283.611568	14.814055
20.503287	1284.876462	14.819072
20.672520	1285.553447	14.824090
20.365706	1283.670539	14.829107
20.875248	1290.681039	14.834125
20.558744	1291.517813	14.839143
20.673550	1274.352245	14.844160
20.770216	1283.077567	14.849178
20.536439	1278.654046	14.854195
20.617917	1287.586179	14.859213
20.247607	1278.092905	14.864231
20.579017	1265.238117	14.869248
20.748880	1283.298695	14.874266
20.909398	1277.566901	14.879283
20.964228	1276.640605	14.884301
20.882862	1281.296972	14.889319
21.091831	1272.798941	14.894336
21.043052	1285.171945	14.899354
20.488024	1287.640409	14.904371
21.001101	1282.755917	14.909389
20.863824	1286.329176	14.914407
20.645406	1285.586007	14.919424
21.427054	1272.777063	14.924442
21.002272	1276.921767	14.929459
21.128362	1273.438423	14.934477
21.138267	1277.589035	14.939495
20.982284	1272.667106	14.944512
20.979801	1271.666633	14.949530
20.714705	1280.728466	14.954547
21.252066	1270.467378	14.959565
20.717927	1284.979129	14.964583
20.775060	1280.404202	14.969600
21.042744	1281.659116	14.974618
21.134145	1302.347630	14.979635
21.444365	1302.464785	14.984653
21.291141	1305.800564	14.989671
21.830273	1302.108228	14.994688
21.430430	1271.175926	14.999706
21.013813	1264.863832	15.004723
21.601080	1261.436934	15.009741
21.462361	1264.962599	15.014759
21.310247	1273.314526	15.019776
21.531681	1261.240789	15.024794
21.510810	1257.322359	15.029811
21.693471	1262.054557	15.034829
21.438587	1265.689366	15.039847
21.535855	1263.454490	15.044864
21.554305	1264.067628	15.049882
21.438699	1266.222169	15.054899
21.515003	1270.076220	15.059917
21.378085	1255.722705	15.064935
21.440424	1264.152555	15.069952
21.552645	1266.850850	15.074970
21.220521	1260.415363	15.079987
21.489127	1270.001295	15.085005
20.987972	1268.983052	15.090023
21.342334	1282.592967	15.095040
21.526818	1282.967873	15.100058
21.639436	1303.724131	15.105075
21.793794	1305.411491	15.110093
21.789606	1300.455217	15.115111
21.600770	1299.859891	15.120128
21.689386	1301.008397	15.125146
21.796636	1297.523831	15.130163
21.718291	1307.808560	15.135181
21.734398	1304.157784	15.140199
21.692406	1298.591712	15.145216
21.942007	1299.657913	15.150234
21.682541	1302.738062	15.155251
21.953476	1304.330381	15.160269
21.807140	1309.828074	15.165287
21.622587	1299.393993	15.170304
21.707121	1303.377184	15.175322
22.072546	1326.857999	15.180339
22.239922	1328.278093	15.185357
22.148056	1320.935292	15.190375
22.434741	1321.310235	15.195392
22.408420	1301.569933	15.200410
22.000465	1301.265701	15.205427
22.079928	1296.028913	15.210445
22.202147	1286.131651	15.215463
22.243719	1283.127751	15.220480
22.380461	1286.309914	15.225498
21.980258	1284.947478	15.230515
22.051788	1287.742645	15.235533
22.193590	1294.421855	15.240551
22.141190	1289.475913	15.245568
22.657208	1290.189472	15.250586
22.214215	1288.911065	15.255603
22.390694	1280.526650	15.260621
21.937496	1284.983681	15.265639
22.397336	1322.015677	15.270656
22.438592	1317.895262	15.275674
22.645337	1318.193272	15.280691
22.585263	1326.149761	15.285709
22.635356	1315.498375	15.290727
22.442685	1305.242966	15.295744
22.356461	1297.802211	15.300762
22.232869	1310.620406	15.305779
22.479227	1332.389285	15.310797
22.534545	1316.212289	15.315815
22.472974	1327.553348	15.320832
22.776584	1319.510249	15.325850
22.420175	1328.017602	15.330867
22.925522	1311.092721	15.335885
22.925394	1315.136356	15.340903
22.663441	1323.896953	15.345920
23.107447	1314.435003	15.350938
22.652865	1326.568261	15.355955
22.555277	1315.295513	15.360973
22.813350	1316.602798	15.365991
22.965624	1320.014845	15.371008
23.310026	1316.826269	15.376026
22.989933	1318.470993	15.381043
22.874332	1319.180487	15.386061
23.066343	1328.087094	15.391079
23.044331	1320.794354	15.396096
22.983021	1299.208743	15.401114
22.805376	1302.863665	15.406131
22.784663	1312.102419	15.411149
23.001073	1309.557735	15.416167
22.948835	1321.270024	15.421184
23.147916	1310.694398	15.426202
22.876349	1308.823769	15.431219
23.036525	1319.400337	15.436237
23.120420	1319.409248	15.441255
23.026802	1314.080800	15.446272
23.131110	1315.853192	15.451290
23.253415	1311.887666	15.456307
23.338909	1309.951534	15.461325
23.562034	1312.702955	15.466343
23.051271	1314.432527	15.471360
23.501482	1316.302063	15.476378
23.101747	1315.820317	15.481395
22.989204	1320.030737	15.486413
23.290723	1306.543157	15.491431
22.844136	1318.364702	15.496448
23.305406	1313.205144	15.501466
23.199523	1314.020889	15.506483
23.083178	1316.496769	15.511501
23.408764	1337.989808	15.516519
23.173997	1343.193119	15.521536
23.361996	1341.436470	15.526554
23.576327	1340.925082	15.531571
22.981092	1345.775036	15.536589
22.667506	1345.534525	15.541607
22.732713	1346.428871	15.546624
23.161956	1353.912640	15.551642
23.095780	1373.348350	15.556659
23.388165	1374.657252	15.561677
23.694632	1362.606779	15.566695
23.422915	1368.296841	15.571712
23.582944	1367.934170	15.576730
24.164807	1369.039744	15.581747
24.029848	1363.994250	15.586765
24.232534	1368.530681	15.591783
23.824851	1371.317275	15.596800
24.244372	1359.887199	15.601818
24.226429	1368.595097	15.606835
23.878385	1359.003816	15.611853
24.127331	1368.243308	15.616871
23.931473	1376.527531	15.621888
24.240234	1369.135229	15.626906
24.410429	1379.045714	15.631923
24.384613	1372.571369	15.636941
24.352763	1364.715554	15.641959
24.326267	1354.168910	15.646976
24.202665	1343.080139	15.651994
23.999274	1340.771729	15.657011
24.055298	1339.153408	15.662029
24.295205	1332.107097	15.667047
24.002414	1339.268714	15.672064
24.178803	1324.642525	15.677082
24.156629	1331.628531	15.682099
24.053545	1343.832238	15.687117
24.462064	1354.813980	15.692135
24.102456	1371.354138	15.697152
24.291429	1369.237340	15.702170
24.186403	1365.406598	15.707187
24.082433	1376.719272	15.712205
23.954280	1369.973891	15.717223
23.862245	1374.525372	15.722240
24.585175	1370.807764	15.727258
24.239406	1365.582377	15.732275
23.920628	1366.986374	15.737293
24.318666	1379.494046	15.742311
24.331846	1393.354706	15.747328
24.445173	1396.294144	15.752346
24.507938	1404.877521	15.757363
24.412899	1399.788219	15.762381
24.760446	1395.506158	15.767399
24.742125	1409.412583	15.772416
24.752006	1394.462716	15.777434
24.978164	1391.026579	15.782451
24.730084	1391.520406	15.787469
25.453851	1404.241749	15.792487
25.001714	1399.743469	15.797504
24.808800	1374.064365	15.802522
24.860397	1372.457401	15.807539
24.577154	1363.554516	15.812557
25.150884	1370.927814	15.817575
24.849203	1371.461203	15.822592
24.735807	1374.888628	15.827610
24.791640	1382.332955	15.832627
24.765789	1397.601237	15.837645
24.965654	1396.047118	15.842663
25.103000	1395.129026	15.847680
25.118251	1395.485255	15.852698
24.848209	1391.459369	15.857715
25.030215	1398.465001	15.862733
25.125075	1394.141444	15.867751
24.912869	1398.968660	15.872768
25.064487	1394.286563	15.877786
25.139548	1389.023309	15.882803
24.718441	1396.676954	15.887821
25.361639	1393.205750	15.892839
24.916758	1398.287723	15.897856
25.032600	1379.875398	15.902874
24.932513	1382.912101	15.907891
25.047720	1401.822474	15.912909
25.471369	1404.553960	15.917927
25.414434	1424.179715	15.922944
25.502756	1413.974042	15.927962
25.731003	1398.284842	15.932979
25.191877	1405.023094	15.937997
25.695617	1394.053413	15.943015
25.312719	1393.887732	15.948032
25.594842	1414.579126	15.953050
25.790244	1405.276690	15.958067
25.501013	1400.660163	15.963085
25.632182	1378.481298	15.968103
25.603506	1387.664729	15.973120
25.602210	1398.101918	15.978138
25.652608	1403.574415	15.983155
25.939577	1414.532987	15.988173
26.127257	1398.590292	15.993191
25.807392	1391.269586	15.998208
25.689205	1381.541304	16.003226
25.861999	1387.993615	16.008243
25.814073	1378.979599	16.013261
25.537974	1372.167735	16.018279
25.584045	1387.226710	16.023296
25.922947	1410.877958	16.028314
25.952798	1416.224346	16.033331
25.780470	1415.009448	16.038349
25.944621	1413.985168	16.043367
26.008232	1420.489587	16.048384
25.841530	1411.866976	16.053402
25.973582	1415.620526	16.058419
25.630853	1419.340547	16.063437
26.028020	1410.688916	16.068455
25.854363	1421.533880	16.073472
26.292809	1405.997112	16.078490
26.109657	1415.120864	16.083507
26.101466	1420.058050	16.088525
26.411742	1410.057200	16.093543
26.008585	1415.386774	16.098560
26.202252	1419.239574	16.103578
26.459716	1409.995767	16.108595
26.101074	1415.976549	16.113613
26.219087	1416.442549	16.118631
26.422987	1420.419822	16.123648
26.306444	1430.367295	16.128666
26.464988	1434.330023	16.133683
26.401254	1441.452652	16.138701
26.904348	1443.905110	16.143719
26.692785	1430.370540	16.148736
26.716921	1428.748229	16.153754
26.380445	1409.755005	16.158771
26.156384	1423.929268	16.163789
26.212099	1424.695088	16.168807
26.495048	1425.479450	16.173824
26.754574	1444.049930	16.178842
26.811899	1442.536486	16.183859
26.808286	1452.657605	16.188877
26.924109	1447.670626	16.193895
26.720480	1443.963624	16.198912
26.604989	1450.244737	16.203930
26.784896	1440.499237	16.208947
26.786473	1451.527240	16.213965
26.980224	1434.841289	16.218983
26.942816	1443.059998	16.224000
26.653110	1443.466035	16.229018
26.728382	1432.622245	16.234035
26.481229	1434.099439	16.239053
26.730624	1439.155653	16.244071
26.841122	1447.978177	16.249088
26.927708	1436.577871	16.254106
27.187365	1439.162868	16.259123
26.929108	1437.529556	16.264141
26.915275	1426.614485	16.269159
27.119544	1443.270165	16.274176
27.544671	1460.994519	16.279194
27.398647	1444.483195	16.284211
27.055821	1442.284611	16.289229
26.956173	1441.306484	16.294247
27.132720	1438.725065	16.299264
27.279183	1462.110009	16.304282
27.720301	1458.955610	16.309299
27.624090	1458.987988	16.314317
27.913069	1429.587357	16.319335
27.421947	1435.347949	16.324352
27.190782	1426.634030	16.329370
27.807816	1422.471969	16.334387
27.314788	1421.232522	16.339405
27.447461	1417.668149	16.344423
27.548503	1422.799064	16.349440
27.510178	1429.057969	16.354458
27.504139	1420.686715	16.359475
27.579945	1431.839818	16.364493
27.644649	1445.141106	16.369511
27.956363	1448.592768	16.374528
27.784010	1445.020734	16.379546
27.718369	1425.368256	16.384563
27.679132	1431.413958	16.389581
27.963238	1458.038271	16.394599
28.225071	1439.786564	16.399616
27.593163	1434.631074	16.404634
27.394879	1430.480147	16.409651
27.416330	1441.377908	16.414669
27.648580	1454.073647	16.419687
27.868883	1455.206897	16.424704
27.788698	1460.620493	16.429722
27.826888	1464.815883	16.434739
27.785345	1452.029857	16.439757
27.827688	1462.212079	16.444775
28.037715	1456.588948	16.449792
27.872464	1456.609904	16.454810
28.159549	1467.557473	16.459827
27.965201	1482.319116	16.464845
28.018541	1478.869793	16.469863
28.150441	1488.758729	16.474880
28.220640	1490.862520	16.479898
28.403792	1491.672628	16.484915
28.332302	1484.071496	16.489933
28.253707	1484.046246	16.494951
28.287081	1489.956564	16.499968
28.360385	1487.196755	16.504986
28.492325	1486.021713	16.510003
28.405332	1489.788649	16.515021
28.438428	1478.417818	16.520039
28.720306	1490.239564	16.525056
28.575449	1487.426844	16.530074
28.461273	1482.781756	16.535091
28.779891	1483.750947	16.540109
28.704878	1480.210253	16.545127
28.917590	1489.819141	16.550144
28.711458	1499.469698	16.555162
28.978083	1482.730122	16.560179
28.728508	1484.524014	16.565197
28.527446	1476.764206	16.570215
28.480752	1474.492863	16.575232
28.557662	1485.409243	16.580250
28.829406	1478.774867	16.585267
28.769466	1473.448277	16.590285
28.608784	1479.462107	16.595303
28.774693	1477.373315	16.600320
28.362575	1489.096787	16.605338
28.998337	1478.732502	16.610355
28.761018	1480.775316	16.615373
28.808376	1495.639921	16.620391
29.140569	1496.453545	16.625408
29.083636	1514.959102	16.630426
28.845467	1515.896311	16.635443
28.914262	1517.418136	16.640461
29.144290	1517.695573	16.645479
29.183357	1507.644611	16.650496
28.990865	1513.212987	16.655514
29.489051	1514.821703	16.660531
29.182756	1509.257703	16.665549
29.048534	1513.454830	16.670567
29.421135	1508.704884	16.675584
29.330045	1521.869212	16.680602
29.150403	1507.489850	16.685619
29.346626	1511.940002	16.690637
29.317872	1517.572056	16.695655
29.324741	1504.474484	16.700672
29.354484	1513.494617	16.705690
29.418887	1509.711420	16.710707
29.365053	1518.895150	16.715725
29.774394	1525.301932	16.720743
30.024782	1523.278492	16.725760
29.825117	1521.852977	16.730778
29.472431	1512.419431	16.735795
29.780311	1506.215624	16.740813
29.570095	1523.646875	16.745831
29.873382	1525.201001	16.750848
29.527072	1529.390472	16.755866
29.733961	1525.814597	16.760883
30.012164	1523.431886	16.765901
29.641390	1531.196159	16.770919
29.988133	1516.984881	16.775936
29.909782	1525.678248	16.780954
30.125262	1525.673484	16.785971
30.441015	1530.668179	16.790989
30.196611	1527.334773	16.796007
30.182656	1532.232599	16.801024
29.981501	1524.611739	16.806042
30.181054	1529.122164	16.811059
29.896920	1534.792885	16.816077
29.853048	1531.594229	16.821095
30.260500	1524.278640	16.826112
29.871968	1531.358150	16.831130
29.817629	1522.170331	16.836147
29.966501	1518.305268	16.841165
30.191025	1529.953871	16.846183
30.573064	1522.708616	16.851200
30.205703	1526.576413	16.856218
30.061771	1523.955239	16.861235
30.221693	1539.391556	16.866253
30.236131	1555.972838	16.871271
30.547226	1543.784273	16.876288
30.681453	1552.542708	16.881306
30.226199	1558.486959	16.886323
30.727605	1546.131921	16.891341
30.438706	1549.133924	16.896359
30.748785	1544.704098	16.901376
30.615061	1549.421160	16.906394
30.882476	1546.640284	16.911411
30.852281	1539.623753	16.916429
30.599603	1546.274379	16.921447
30.953446	1549.377812	16.926464
30.774119	1546.478664	16.931482
30.607541	1537.341860	16.936499
30.830044	1544.877800	16.941517
30.709463	1549.615915	16.946535
31.115368	1547.358729	16.951552
30.933710	1545.122080	16.956570
30.542971	1549.802493	16.961587
30.723347	1548.761352	16.966605
30.519926	1549.676681	16.971623
31.241096	1563.817879	16.976640
31.259987	1575.724681	16.981658
31.521657	1582.607208	16.986675
31.423426	1571.342842	16.991693
31.351499	1559.776935	16.996711
31.527383	1545.289184	17.001728
31.321483	1556.018328	17.006746
30.958019	1550.790487	17.011763
31.390095	1543.806994	17.016781
31.186750	1555.130514	17.021799
31.666717	1563.939087	17.026816
31.556248	1549.528178	17.031834
31.571074	1548.616350	17.036851
31.303649	1548.265465	17.041869
31.430403	1558.458207	17.046887
31.451992	1567.554119	17.051904
31.525387	1573.271070	17.056922
31.468888	1570.703736	17.061939
31.987459	1567.750856	17.066957
31.648468	1573.125187	17.071975
31.857394	1568.380031	17.076992
31.743609	1570.795301	17.082010
31.819173	1565.092595	17.087027
31.926204	1558.122660	17.092045
31.600606	1568.082332	17.097063
31.833971	1560.756918	17.102080
31.959799	1565.177977	17.107098
31.722908	1565.129877	17.112115
32.158728	1562.045418	17.117133
31.776135	1570.646196	17.122151
31.874464	1560.275606	17.127168
32.292171	1566.773727	17.132186
32.024836	1559.744809	17.137203
31.826961	1560.547624	17.142221
32.011746	1567.659749	17.147239
32.501488	1557.355561	17.152256
32.143139	1560.640856	17.157274
32.017965	1579.034753	17.162291
32.051868	1564.528917	17.167309
31.692762	1565.294213	17.172327
32.064736	1584.945538	17.177344
32.068153	1603.075333	17.182362
32.179973	1610.060381	17.187379
32.294400	1594.435651	17.192397
32.376630	1599.047954	17.197415
32.306018	1597.449550	17.202432
32.599180	1593.458471	17.207450
32.689729	1593.281860	17.212467
32.653741	1589.618762	17.217485
32.649308	1597.632131	17.222503
32.585291	1580.619183	17.227520
32.920694	1593.645384	17.232538
32.736882	1600.252176	17.237555
33.027166	1591.213635	17.242573
32.770301	1595.272413	17.247591
32.595713	1590.772888	17.252608
32.852110	1591.771854	17.257626
32.918257	1590.131758	17.262643
33.166716	1590.560658	17.267661
32.963270	1593.900665	17.272679
32.653046	1592.048198	17.277696
32.962228	1592.492256	17.282714
32.831189	1594.415567	17.287731
32.880692	1591.837207	17.292749
32.877862	1594.711442	17.297767
32.900041	1587.123909	17.302784
33.250985	1597.816563	17.307802
32.923027	1603.533916	17.312819
33.327449	1596.833475	17.317837
33.083303	1621.650352	17.322855
33.138560	1622.795144	17.327872
33.411529	1612.880436	17.332890
33.331429	1621.190930	17.337907
33.633167	1603.890179	17.342925
33.244104	1622.131111	17.347943
33.519135	1624.243780	17.352960
33.531959	1615.360512	17.357978
33.256124	1616.263012	17.362995
33.363247	1615.056043	17.368013
33.782877	1616.892291	17.373031
33.537462	1613.647406	17.378048
33.560412	1612.547840	17.383066
33.615581	1625.308412	17.388083
33.659885	1613.384522	17.393101
33.682280	1613.762407	17.398119
33.420429	1613.093910	17.403136
33.455238	1610.612844	17.408154
33.429439	1623.089592	17.413171
33.427109	1637.326803	17.418189
33.755743	1639.401289	17.423207
33.547546	1652.968889	17.428224
33.920946	1641.599763	17.433242
34.028000	1644.964049	17.438259
34.193360	1637.175491	17.443277
34.132352	1641.277888	17.448295
33.902911	1643.494201	17.453312
34.096366	1632.212489	17.458330
34.124346	1637.844068	17.463347
34.267311	1627.944930	17.468365
34.256872	1635.011209	17.473383
33.968869	1632.658478	17.478400
34.231298	1635.844939	17.483418
34.026469	1641.438231	17.488435
34.473347	1667.061728	17.493453
34.794231	1670.515075	17.498471
34.639670	1655.284492	17.503488
34.797326	1646.730965	17.508506
34.537927	1631.498837	17.513523
34.749062	1634.417433	17.518541
34.759220	1636.430786	17.523559
34.577676	1631.463365	17.528576
34.870558	1636.834267	17.533594
34.876869	1627.772761	17.538611
34.596046	1626.501967	17.543629
34.453979	1631.256648	17.548647
34.282948	1633.326317	17.553664
34.806579	1644.888182	17.558682
34.952317	1659.813252	17.563699
35.105339	1655.728993	17.568717
35.256440	1653.279680	17.573735
34.939532	1635.231440	17.578752
34.943638	1629.669636	17.583770
34.536677	1629.729748	17.588787
34.872802	1641.190528	17.593805
34.934875	1645.883332	17.598823
35.078957	1656.300017	17.603840
35.147677	1660.013313	17.608858
35.094475	1657.392671	17.613875
35.277204	1649.762829	17.618893
35.419411	1661.905388	17.623911
35.076738	1654.347806	17.628928
35.226388	1660.476344	17.633946
35.228059	1663.068979	17.638963
35.475661	1648.054780	17.643981
35.424626	1649.326771	17.648999
35.051953	1651.179996	17.654016
35.226835	1652.410913	17.659034
35.158881	1658.106772	17.664051
35.683511	1673.741187	17.669069
35.839127	1675.614773	17.674087
35.504131	1670.139895	17.679104
35.785248	1666.545028	17.684122
35.704774	1675.900555	17.689139
35.862971	1685.664816	17.694157
35.892087	1683.516526	17.699175
35.653869	1679.252067	17.704192
36.227109	1685.031910	17.709210
35.604373	1684.753123	17.714227
35.768157	1688.445795	17.719245
36.064976	1684.185619	17.724263
35.682636	1689.519916	17.729280
36.035966	1682.092741	17.734298
35.866938	1681.285097	17.739315
35.934209	1690.064517	17.744333
35.902536	1686.082614	17.749351
35.723993	1680.074069	17.754368
36.057044	1680.726363	17.759386
35.896266	1685.281029	17.764403
35.857892	1693.844279	17.769421
36.336992	1695.853362	17.774439
36.320237	1698.135112	17.779456
36.539335	1703.026364	17.784474
36.256356	1707.409918	17.789491
36.513309	1709.170121	17.794509
36.539443	1707.073692	17.799527
36.333548	1704.390098	17.804544
36.711841	1704.435781	17.809562
36.669128	1698.203036	17.814579
36.673824	1695.255537	17.819597
37.069276	1701.041935	17.824615
36.726649	1702.499699	17.829632
37.054665	1704.243828	17.834650
36.809746	1710.448811	17.839667
36.817286	1697.929236	17.844685
36.937781	1704.534990	17.849703
36.905256	1711.093800	17.854720
37.200840	1711.259830	17.859738
36.754040	1701.819085	17.864755
36.873230	1700.672903	17.869773
36.801526	1708.699809	17.874791
36.850341	1701.743760	17.879808
36.951904	1693.653356	17.884826
37.074150	1707.812966	17.889843
37.006376	1701.911091	17.894861
36.876391	1701.434943	17.899879
36.785910	1705.855770	17.904896
37.015816	1712.074399	17.909914
37.019023	1720.794550	17.914931
37.095318	1727.225162	17.919949
37.278075	1725.457723	17.924967
37.233388	1725.883307	17.929984
37.355101	1723.306770	17.935002
37.759161	1736.307377	17.940019
37.747328	1730.334443	17.945037
37.813690	1722.152413	17.950055
37.747148	1732.405951	17.955072
37.727649	1735.655754	17.960090
37.774367	1722.627386	17.965107
38.018760	1721.730359	17.970125
37.953262	1722.268423	17.975143
37.711904	1731.368323	17.980160
37.727937	1726.715028	17.985178
37.751447	1729.392046	17.990195
37.676208	1730.495428	17.995213
37.963896	1725.083157	18.000231
37.706261	1726.470192	18.005248
37.841913	1715.373539	18.010266
37.758466	1719.821551	18.015283
37.471473	1730.443760	18.020301
37.983764	1728.102638	18.025319
37.575303	1753.549166	18.030336
38.060607	1755.893410	18.035354
38.043922	1744.194038	18.040371
38.256783	1760.133968	18.045389
38.487622	1751.226206	18.050407
38.429408	1750.616164	18.055424
38.450843	1751.652199	18.060442
38.416797	1748.234775	18.065459
38.622843	1753.926328	18.070477
38.284592	1745.241340	18.075495
38.016789	1754.378100	18.080512
38.415009	1747.841395	18.085530
38.627760	1753.579865	18.090547
38.460286	1758.070314	18.095565
38.808949	1769.205142	18.100583
38.517840	1784.465681	18.105600
39.061545	1782.856868	18.110618
39.147892	1779.322702	18.115635
38.943111	1773.829614	18.120653
39.224636	1757.184904	18.125671
38.915717	1745.681444	18.130688
38.743947	1746.631903	18.135706
39.018449	1749.719358	18.140723
38.991928	1781.790166	18.145741
39.090513	1778.851345	18.150759
38.916177	1783.849368	18.155776
39.307564	1788.625375	18.160794
39.182555	1781.244332	18.165811
39.165502	1780.310203	18.170829
39.327556	1768.605877	18.175847
39.508879	1770.131766	18.180864
39.357349	1774.704219	18.185882
39.494166	1776.199673	18.190899
39.676375	1773.353123	18.195917
39.844946	1775.538912	18.200935
39.171766	1769.693560	18.205952
39.250771	1776.006829	18.210970
39.268853	1769.684688	18.215987
39.275263	1778.016202	18.221005
39.541667	1772.959356	18.226023
39.615404	1776.889147	18.231040
39.632952	1780.146418	18.236058
39.735589	1769.474619	18.241075
39.509741	1770.062409	18.246093
39.826910	1770.386664	18.251111
39.848199	1762.395305	18.256128
39.873563	1763.061053	18.261146
39.878555	1765.248680	18.266163
39.595933	1769.880587	18.271181
40.016320	1776.811766	18.276199
40.009113	1791.900412	18.281216
40.192438	1799.005997	18.286234
40.291657	1794.948111	18.291251
40.324856	1797.937281	18.296269
40.275125	1791.808991	18.301287
40.274362	1797.453252	18.306304
40.177427	1801.283710	18.311322
40.676956	1795.961981	18.316339
40.413607	1795.313996	18.321357
40.554573	1798.178086	18.326375
40.203942	1798.037574	18.331392
39.969563	1791.135764	18.336410
40.171648	1791.986063	18.341427
40.132884	1801.618990	18.346445
40.367801	1794.191648	18.351463
40.548198	1809.880923	18.356480
40.528346	1819.087363	18.361498
40.980127	1830.770481	18.366515
40.735093	1839.213257	18.371533
40.928082	1828.966984	18.376551
41.016887	1821.709426	18.381568
40.812653	1825.113581	18.386586
40.834429	1817.020748	18.391603
40.981214	1835.152907	18.396621
41.225262	1826.492495	18.401639
40.993246	1827.491886	18.406656
40.835305	1836.673918	18.411674
40.969509	1822.032775	18.416691
40.963569	1829.619401	18.421709
40.793074	1822.254121	18.426727
41.075247	1821.857477	18.431744
40.789554	1825.557737	18.436762
41.109565	1827.480937	18.441779
41.195117	1850.510638	18.446797
41.214714	1846.677092	18.451815
41.850061	1857.907111	18.456832
41.788859	1855.122816	18.461850
41.936892	1848.239073	18.466867
41.681272	1845.288114	18.471885
42.144565	1832.993668	18.476903
42.066925	1851.766012	18.481920
41.226706	1838.546363	18.486938
41.831813	1832.436007	18.491955
41.269847	1840.210971	18.496973
41.439600	1836.463623	18.501991
41.755735	1837.401363	18.507008
41.681178	1842.891713	18.512026
42.330099	1835.948426	18.517043
41.723020	1834.881709	18.522061
42.142299	1833.132449	18.527079
42.066502	1831.250265	18.532096
42.114101	1843.841621	18.537114
42.471406	1840.300849	18.542131
42.321362	1840.863517	18.547149
42.258886	1837.776913	18.552167
42.229791	1849.185225	18.557184
42.134833	1840.448954	18.562202
42.461045	1825.164733	18.567219
42.166142	1829.577453	18.572237
42.363894	1848.799893	18.577255
42.503379	1856.623295	18.582272
42.408269	1875.389107	18.587290
42.867562	1863.256500	18.592307
42.703591	1869.290117	18.597325
42.832201	1871.102450	18.602343
42.896305	1853.265169	18.607360
42.618730	1850.720742	18.612378
42.760342	1847.186875	18.617395
42.839494	1866.996586	18.622413
42.707158	1857.475434	18.627431
42.861257	1862.455422	18.632448
42.699203	1868.456443	18.637466
42.718787	1859.857119	18.642483
42.926399	1870.041823	18.647501
42.896318	1858.223923	18.652519
43.018357	1866.962310	18.657536
42.611432	1866.938765	18.662554
43.097430	1857.247327	18.667571
43.348400	1865.376484	18.672589
43.355527	1865.125871	18.677607
43.341118	1870.712381	18.682624
43.424102	1880.409283	18.687642
43.596963	1874.666961	18.692659
43.426353	1869.545509	18.697677
43.529992	1872.031182	18.702695
43.464566	1866.236717	18.707712
43.138524	1887.683900	18.712730
43.827053	1880.228398	18.717747
43.687922	1873.824136	18.722765
43.557430	1876.341219	18.727783
43.760108	1885.071998	18.732800
43.531615	1882.323611	18.737818
43.788155	1869.892260	18.742835
43.689242	1886.445589	18.747853
43.466359	1883.810828	18.752871
43.818787	1886.863783	18.757888
43.646927	1900.543101	18.762906
43.959911	1907.380094	18.767923
43.800964	1918.399137	18.772941
44.117789	1906.178045	18.777959
44.425158	1910.198182	18.782976
44.069415	1915.399041	18.787994
44.374318	1895.244030	18.793011
44.276290	1908.541709	18.798029
44.524460	1907.837529	18.803047
44.394216	1899.770956	18.808064
44.144724	1904.754276	18.813082
44.504606	1903.693485	18.818099
44.442695	1901.823367	18.823117
44.198856	1899.037753	18.828135
44.498426	1917.746857	18.833152
44.441507	1927.930242	18.838170
44.598526	1932.634802	18.843187
44.693669	1941.136168	18.848205
45.017288	1929.468990	18.853223
45.208812	1926.234697	18.858240
44.828662	1937.788677	18.863258
44.652724	1920.961348	18.868275
45.088080	1919.108646	18.873293
45.172703	1921.220937	18.878311
45.359089	1924.015939	18.883328
45.317853	1926.865484	18.888346
45.263358	1925.559820	18.893363
45.539352	1916.673828	18.898381
44.969958	1924.042036	18.903399
45.304289	1923.419079	18.908416
45.117096	1932.416456	18.913434
45.363382	1918.778827	18.918451
45.320892	1921.135131	18.923469
45.175781	1925.224930	18.928487
45.233195	1919.438685	18.933504
45.258137	1922.021219	18.938522
45.320269	1936.200028	18.943539
45.433598	1947.931294	18.948557
45.348302	1945.445420	18.953575
45.718796	1948.726281	18.958592
45.325164	1951.677171	18.963610
45.825360	1952.544939	18.968627
46.230766	1951.895670	18.973645
45.746118	1945.373890	18.978663
46.143432	1949.647254	18.983680
45.927868	1947.560227	18.988698
45.969387	1943.847429	18.993715
46.128791	1944.781356	18.998733
46.041161	1957.795107	19.003751
46.250160	1941.003345	19.008768
46.496137	1944.583098	19.013786
46.184935	1939.548431	19.018803
46.351240	1942.785681	19.023821
46.424552	1950.712970	19.028839
46.661408	1944.826006	19.033856
46.566877	1939.904926	19.038874
46.617594	1952.559628	19.043891
46.941076	1939.989810	19.048909
46.429597	1943.974233	19.053927
46.413722	1949.228768	19.058944
46.394519	1944.692044	19.063962
46.690822	1960.700470	19.068979
46.978261	1970.202636	19.073997
46.805964	1972.737468	19.079015
47.064750	1972.860180	19.084032
46.880115	1976.543578	19.089050
46.780051	1977.133420	19.094067
46.979033	1980.465267	19.099085
46.609874	1977.114981	19.104103
46.815771	1974.274715	19.109120
46.856539	1973.774473	19.114138
46.955462	1968.574985	19.119155
47.261858	1969.771598	19.124173
47.004368	1966.292439	19.129191
47.203293	1986.775150	19.134208
47.371142	1996.607691	19.139226
47.621393	1997.860824	19.144243
47.504412	2002.231396	19.149261
47.351610	2002.978758	19.154279
47.951328	1995.496348	19.159296
47.592271	1993.264738	19.164314
47.684797	1998.398238	19.169331
47.564417	1998.668049	19.174349
47.666210	1999.807738	19.179367
47.894348	2002.666122	19.184384
47.877019	1995.290800	19.189402
47.970493	1993.404637	19.194419
48.227525	1995.230995	19.199437
48.184692	1997.787936	19.204455
48.277129	1992.847947	19.209472
47.984792	1987.775505	19.214490
48.141517	1995.163106	19.219507
48.174137	1989.462419	19.224525
47.546132	1993.911534	19.229543
47.548625	1996.854642	19.234560
47.886332	2009.146841	19.239578
48.173738	2018.065838	19.244595
48.523697	2030.617024	19.249613
48.269253	2028.101418	19.254631
48.595234	2022.435105	19.259648
48.683904	2019.375252	19.264666
48.749863	2013.402540	19.269683
48.848375	2022.704883	19.274701
48.702698	2019.194637	19.279719
48.525584	2008.927526	19.284736
48.727250	2020.635983	19.289754
48.264789	2015.737890	19.294771
48.566066	2023.417330	19.299789
48.837540	2031.275893	19.304807
48.758313	2038.892841	19.309824
48.936964	2045.597387	19.314842
48.650481	2037.077675	19.319859
48.918939	2055.725560	19.324877
48.897175	2051.080577	19.329895
49.264981	2042.496433	19.334912
49.125108	2045.023753	19.339930
49.129898	2040.979046	19.344947
49.321049	2042.302179	19.349965
49.282911	2065.976001	19.354983
49.934533	2062.641042	19.360000
49.637710	2055.268970	19.365018
49.685583	2043.206771	19.370035
49.667835	2040.930364	19.375053
49.644597	2046.973467	19.380071
49.808325	2058.266415	19.385088
49.962439	2071.527685	19.390106
49.633210	2068.755758	19.395123
49.961641	2070.706532	19.400141
49.884003	2078.306113	19.405159
50.165256	2073.266006	19.410176
49.866678	2074.932643	19.415194
49.878830	2079.191552	19.420211
50.349515	2070.083948	19.425229
50.162437	2080.334214	19.430247
50.515516	2067.908795	19.435264
50.550867	2070.032596	19.440282
50.030633	2068.445459	19.445299
50.522608	2059.141647	19.450317
50.174800	2070.801196	19.455335
50.158005	2065.964463	19.460352
50.513260	2072.891385	19.465370
50.525948	2058.153970	19.470387
50.599866	2057.828740	19.475405
50.609403	2068.601566	19.480423
50.480102	2053.356179	19.485440
50.697705	2076.808050	19.490458
50.297452	2092.965186	19.495475
50.691509	2089.907603	19.500493
50.498736	2102.884527	19.505511
50.755227	2096.126634	19.510528
51.207872	2088.517319	19.515546
50.665898	2096.898688	19.520563
51.162386	2093.996600	19.525581
51.070256	2104.095182	19.530599
50.928697	2098.649200	19.535616
51.359905	2104.221203	19.540634
51.332357	2120.621468	19.545651
51.529605	2119.410393	19.550669
51.559647	2121.445127	19.555687
51.537458	2117.124571	19.560704
52.234057	2107.064548	19.565722
51.666051	2105.437865	19.570739
51.865614	2077.113070	19.575757
51.609423	2090.157151	19.580775
51.554481	2081.870185	19.585792
51.730606	2082.358884	19.590810
51.429471	2106.877526	19.595827
52.017647	2103.505607	19.600845
51.428562	2114.358691	19.605863
51.966305	2110.361311	19.610880
51.911922	2112.871169	19.615898
51.949941	2117.173447	19.620915
52.155633	2110.028314	19.625933
51.986802	2114.320881	19.630951
51.869256	2105.029391	19.635968
52.102129	2110.770773	19.640986
52.272083	2113.593522	19.646003
52.331194	2117.041614	19.651021
52.282499	2135.177104	19.656039
52.379736	2132.697054	19.661056
52.750143	2141.236498	19.666074
52.521885	2141.463712	19.671091
52.976713	2130.234299	19.676109
53.063775	2129.932287	19.681127
52.891819	2132.897754	19.686144
53.166705	2131.610075	19.691162
52.694825	2114.007508	19.696179
52.607657	2117.064855	19.701197
52.932132	2122.624979	19.706215
52.960678	2126.607401	19.711232
53.258595	2123.440318	19.716250
52.652124	2126.177817	19.721267
53.086449	2125.917227	19.726285
52.867107	2124.756099	19.731303
53.123322	2132.776078	19.736320
53.538175	2128.046519	19.741338
53.276360	2123.768513	19.746355
53.454275	2122.664953	19.751373
53.094278	2121.520574	19.756391
53.340082	2137.341290	19.761408
53.793764	2156.403329	19.766426
53.289043	2154.584114	19.771443
53.548268	2162.668959	19.776461
53.524489	2154.857269	19.781479
53.561152	2158.344115	19.786496
53.773873	2141.348784	19.791514
53.757532	2149.541360	19.796531
53.820263	2154.684559	19.801549
53.944381	2152.628762	19.806567
54.104384	2161.756673	19.811584
54.202198	2172.760629	19.816602
54.003047	2173.383387	19.821619
54.396442	2182.347556	19.826637
54.400490	2195.695340	19.831655
54.427301	2183.644975	19.836672
54.880796	2183.376493	19.841690
54.705264	2193.350739	19.846707
54.599911	2171.323589	19.851725
54.301034	2168.487972	19.856743
54.322309	2172.322016	19.861760
54.431607	2169.275259	19.866778
54.345186	2181.406212	19.871795
54.334199	2169.204640	19.876813
54.516614	2179.468510	19.881831
54.313556	2182.660561	19.886848
54.738816	2192.632364	19.891866
54.453474	2207.728604	19.896883
54.607474	2204.101673	19.901901
55.202969	2204.332115	19.906919
55.027329	2199.956194	19.911936
55.146328	2203.903414	19.916954
55.303221	2204.825569	19.921971
55.284938	2197.458378	19.926989
55.586978	2209.424381	19.932007
55.611247	2202.660924	19.937024
55.591104	2200.982863	19.942042
55.724891	2197.677157	19.947059
55.794107	2198.895859	19.952077
55.554460	2194.679519	19.957095
55.587123	2195.297037	19.962112
55.626206	2192.725613	19.967130
55.457984	2210.764223	19.972147
56.001326	2202.769624	19.977165
55.932977	2217.345415	19.982183
56.080359	2220.079601	19.987200
56.328607	2219.123844	19.992218
56.203589	2224.976769	19.997235
56.389070	2216.879112	20.002253
56.045011	2195.406483	20.007271
56.500919	2199.781248	20.012288
56.377889	2190.020776	20.017306
56.330584	2192.012795	20.022323
56.400708	2207.647872	20.027341
56.233411	2217.744778	20.032359
56.329340	2222.513455	20.037376
56.353293	2223.087339	20.042394
56.252133	2213.846810	20.047411
56.297357	2224.779777	20.052429
56.653584	2222.278368	20.057447
56.445067	2225.603011	20.062464
56.446911	2226.818087	20.067482
56.430493	2238.317300	20.072499
56.765200	2251.195173	20.077517
56.936161	2245.160142	20.082535
56.698779	2242.614517	20.087552
57.372502	2245.871315	20.092570
57.130433	2246.756853	20.097587
56.988687	2248.923920	20.102605
57.001123	2242.385018	20.107623
56.604192	2261.141536	20.112640
57.572877	2264.582447	20.117658
57.456670	2280.849910	20.122675
57.333662	2273.606082	20.127693
57.658504	2275.115785	20.132711
57.370707	2275.900427	20.137728
57.631484	2275.264221	20.142746
57.547599	2263.932022	20.147763
57.443871	2282.824939	20.152781
58.063919	2293.720438	20.157799
58.001748	2294.310132	20.162816
57.959283	2293.115037	20.167834
58.049809	2310.219745	20.172851
58.075072	2293.815805	20.177869
58.321896	2298.212357	20.182887
58.318615	2302.088480	20.187904
58.555181	2294.433284	20.192922
58.295323	2282.711292	20.197939
58.152603	2294.008407	20.202957
58.345291	2282.651550	20.207975
58.482489	2290.609595	20.212992
58.746557	2291.370750	20.218010
58.529321	2293.388304	20.223027
58.563180	2283.419383	20.228045
58.863581	2291.977566	20.233063
58.587923	2300.366014	20.238080
58.768877	2294.026977	20.243098
58.826165	2308.216574	20.248115
58.724898	2313.331618	20.253133
59.406823	2318.529030	20.258151
59.175851	2324.927999	20.263168
59.496723	2312.837795	20.268186
58.905242	2319.307360	20.273203
59.148391	2309.813633	20.278221
59.648322	2306.359216	20.283239
59.562743	2307.800931	20.288256
59.822093	2299.123161	20.293274
59.456451	2309.383994	20.298291
59.109120	2306.735870	20.303309
59.583128	2312.091249	20.308327
59.387631	2310.518723	20.313344
59.759031	2314.545511	20.318362
59.341348	2315.927158	20.323379
59.300487	2293.639197	20.328397
59.983772	2307.147050	20.333415
59.645783	2314.110107	20.338432
59.527426	2325.656740	20.343450
60.095824	2334.269666	20.348467
60.069149	2344.241062	20.353485
60.224299	2329.309782	20.358503
60.006917	2336.809365	20.363520
60.165535	2334.486842	20.368538
60.099986	2335.567210	20.373555
60.185994	2335.752334	20.378573
60.586033	2340.095037	20.383591
60.029768	2356.047539	20.388608
60.187253	2353.050456	20.393626
60.756992	2373.032873	20.398643
60.426844	2366.677490	20.403661
60.534774	2368.259265	20.408679
60.555504	2374.834948	20.413696
61.013308	2362.799040	20.418714
60.803961	2379.177068	20.423731
60.807536	2390.689231	20.428749
61.583971	2390.042209	20.433767
61.255827	2398.193144	20.438784
61.172398	2398.449572	20.443802
61.321838	2400.465005	20.448819
61.190936	2408.049339	20.453837
61.450886	2393.043400	20.458855
61.634178	2405.658260	20.463872
61.567600	2401.916369	20.468890
61.512306	2393.998554	20.473907
61.447255	2392.887886	20.478925
61.513886	2388.296889	20.483943
61.561824	2387.783837	20.488960
61.874659	2389.153421	20.493978
61.770404	2384.914850	20.498995
61.771406	2397.774968	20.504013
61.897370	2401.543544	20.509031
61.834496	2413.883172	20.514048
62.182426	2408.178646	20.519066
62.395050	2414.474820	20.524083
62.317148	2417.203950	20.529101
62.702996	2410.036781	20.534119
62.510734	2415.361565	20.539136
62.769769	2414.664229	20.544154
62.795744	2412.656110	20.549171
62.622127	2424.821150	20.554189
62.822361	2407.781334	20.559207
62.647754	2418.735610	20.564224
62.802012	2406.912414	20.569242
62.784081	2414.800891	20.574259
62.786323	2416.052134	20.579277
62.753160	2409.534672	20.584295
62.774175	2412.169311	20.589312
62.474833	2407.941321	20.594330
62.772140	2417.528347	20.599347
62.833416	2415.149660	20.604365
63.107904	2437.139453	20.609383
62.816817	2448.478126	20.614400
62.829265	2441.442525	20.619418
63.298704	2431.406448	20.624435
62.884471	2445.092839	20.629453
63.408297	2454.580058	20.634471
63.487311	2470.308807	20.639488
63.558334	2473.899487	20.644506
63.756445	2467.892952	20.649523
63.618186	2474.976999	20.654541
63.518918	2468.763917	20.659559
63.807961	2464.394391	20.664576
63.973303	2463.375949	20.669594
64.161267	2460.622017	20.674611
63.798213	2460.566415	20.679629
63.886422	2476.559181	20.684647
64.282615	2487.700653	20.689664
64.122584	2491.561982	20.694682
64.449072	2492.829721	20.699699
64.165062	2492.803967	20.704717
64.744657	2494.524330	20.709735
64.619973	2495.872926	20.714752
64.387150	2484.807679	20.719770
64.661987	2485.376922	20.724787
64.439868	2488.719024	20.729805
64.462496	2480.137355	20.734823
64.756423	2498.839044	20.739840
64.760687	2514.412093	20.744858
64.923701	2513.570791	20.749875
64.927566	2516.509834	20.754893
65.092118	2512.701181	20.759911
65.290945	2519.809459	20.764928
65.438482	2515.780995	20.769946
65.740866	2503.167952	20.774963
65.691843	2507.918745	20.779981
65.567730	2508.879483	20.784999
65.680309	2515.227465	20.790016
65.579672	2498.166409	20.795034
65.629645	2505.417577	20.800051
65.640978	2507.091111	20.805069
65.557595	2501.531640	20.810087
65.760637	2504.647593	20.815104
65.645459	2508.501121	20.820122
65.745953	2516.569473	20.825139
65.768772	2545.503047	20.830157
65.886447	2538.548036	20.835175
66.053790	2537.371397	20.840192
66.033016	2539.198064	20.845210
66.434105	2535.750680	20.850227
66.224920	2535.124416	20.855245
66.334806	2529.124168	20.860263
66.261390	2552.649657	20.865280
66.268670	2558.069458	20.870298
66.567457	2560.319662	20.875315
66.442740	2573.201685	20.880333
66.938019	2561.833397	20.885351
67.121257	2560.343128	20.890368
66.958005	2564.614033	20.895386
67.132789	2552.165727	20.900403
66.710626	2565.251413	20.905421
67.260812	2560.019867	20.910439
67.399269	2559.862099	20.915456
67.327826	2565.561427	20.920474
67.331826	2554.577064	20.925491
67.193746	2554.526801	20.930509
67.443939	2558.145565	20.935527
67.210326	2572.197664	20.940544
67.361467	2584.884120	20.945562
67.574308	2580.972792	20.950579
67.754698	2586.987967	20.955597
67.540551	2588.933991	20.960615
67.679798	2589.333336	20.965632
67.558717	2588.090977	20.970650
68.023124	2570.863636	20.975667
67.942949	2591.706834	20.980685
67.729066	2581.766457	20.985703
68.078923	2601.234366	20.990720
68.204695	2614.075619	20.995738
68.430243	2607.343286	21.000755
68.460533	2615.068001	21.005773
68.675703	2603.800102	21.010791
68.798493	2604.730476	21.015808
68.737250	2602.312956	21.020826
68.930882	2601.187475	21.025843
68.688928	2609.848650	21.030861
68.700353	2606.917187	21.035879
69.068339	2607.214760	21.040896
69.018055	2614.034547	21.045914
69.037329	2600.644054	21.050931
68.663711	2601.744250	21.055949
68.803357	2597.393470	21.060967
69.215594	2600.832524	21.065984
68.665940	2609.597299	21.071002
69.083691	2601.969881	21.076019
69.244215	2598.526806	21.081037
69.324022	2615.291916	21.086055
69.028228	2625.930168	21.091072
69.229202	2623.092370	21.096090
69.494476	2636.247967	21.101107
69.314517	2627.546554	21.106125
69.313622	2642.801119	21.111143
69.574797	2660.413609	21.116160
69.709407	2662.098282	21.121178
69.952853	2653.613284	21.126195
69.888915	2658.947061	21.131213
69.698549	2662.981938	21.136231
70.505859	2669.212422	21.141248
70.148650	2691.706154	21.146266
70.539021	2675.798918	21.151283
70.626943	2685.692742	21.156301
70.555941	2680.353784	21.161319
70.712364	2681.532525	21.166336
70.589732	2674.181957	21.171354
70.648827	2675.910999	21.176371
70.852464	2683.398848	21.181389
70.948450	2686.976595	21.186407
71.157789	2670.352085	21.191424
70.871821	2678.380850	21.196442
70.810168	2675.944096	21.201459
70.771648	2669.245728	21.206477
70.929602	2680.068465	21.211495
70.867940	2697.425903	21.216512
71.256318	2704.162611	21.221530
71.077083	2701.857874	21.226547
70.900447	2704.068562	21.231565
71.102442	2710.695531	21.236583
71.458346	2716.386102	21.241600
71.327777	2729.834147	21.246618
71.924409	2738.161551	21.251635
72.100577	2730.801143	21.256653
71.918203	2725.912437	21.261671
72.252522	2726.025431	21.266688
72.237897	2730.339139	21.271706
72.689388	2718.503593	21.276723
72.660762	2716.593231	21.281741
72.437049	2724.249156	21.286759
72.363547	2728.440318	21.291776
72.493786	2728.295716	21.296794
72.456418	2731.497110	21.301811
72.638380	2721.100505	21.306829
72.505367	2728.041880	21.311847
72.497033	2727.289902	21.316864
72.206147	2725.059515	21.321882
72.090213	2720.800342	21.326899
72.638702	2743.211208	21.331917
72.541124	2761.388579	21.336935
72.903424	2756.755109	21.341952
73.125380	2760.419137	21.346970
72.890510	2751.638151	21.351987
73.057937	2758.160623	21.357005
73.312806	2765.077678	21.362023
73.663333	2758.184084	21.367040
73.513151	2788.585197	21.372058
73.675210	2788.886098	21.377075
73.709176	2777.802929	21.382093
73.730829	2782.184668	21.387111
74.041591	2778.115975	21.392128
73.491258	2774.963944	21.397146
73.854500	2771.140109	21.402163
74.012076	2779.030278	21.407181
74.044429	2771.826680	21.412199
74.457343	2775.216649	21.417216
74.249527	2778.564717	21.422234
74.225137	2767.364435	21.427251
74.436790	2775.474786	21.432269
74.167476	2773.894725	21.437287
74.163486	2770.549661	21.442304
74.356091	2794.758680	21.447322
74.434001	2806.106711	21.452339
74.597986	2805.564429	21.457357
74.220151	2806.652934	21.462375
74.876168	2810.842061	21.467392
74.579168	2823.929917	21.472410
74.779318	2823.787147	21.477427
75.100053	2829.496170	21.482445
75.021107	2833.636687	21.487463
74.905362	2833.075673	21.492480
74.931953	2840.665096	21.497498
75.077260	2832.529862	21.502515
75.192553	2850.090302	21.507533
75.178687	2855.646765	21.512551
75.631694	2855.722432	21.517568
75.741009	2859.688547	21.522586
75.901840	2862.172213	21.527603
75.933582	2851.426742	21.532621
75.740365	2863.280618	21.537639
75.986972	2847.945163	21.542656
75.985607	2863.594686	21.547674
75.906252	2871.864196	21.552691
76.064297	2884.790690	21.557709
76.287238	2878.512584	21.562727
76.329798	2880.251664	21.567744
76.173536	2883.331012	21.572762
76.231179	2879.764727	21.577779
76.305668	2872.848198	21.582797
76.653149	2897.539237	21.587815
76.852394	2900.525984	21.592832
76.446948	2916.164387	21.597850
76.883779	2913.475543	21.602867
76.753347	2907.088506	21.607885
77.035298	2908.235302	21.612903
77.326962	2907.747110	21.617920
77.173274	2911.870474	21.622938
77.353999	2904.791500	21.627955
77.252299	2904.004551	21.632973
77.560151	2922.699730	21.637991
77.609800	2916.249861	21.643008
77.756993	2941.633091	21.648026
77.712122	2938.332540	21.653043
77.983503	2926.783281	21.658061
77.814542	2941.762188	21.663079
77.829073	2944.174772	21.668096
77.730882	2933.125536	21.673114
77.826371	2943.844022	21.678131
78.214402	2929.752770	21.683149
78.068366	2925.791414	21.688167
78.359872	2930.649835	21.693184
78.484056	2935.380798	21.698202
78.186303	2934.286105	21.703219
78.410840	2931.657142	21.708237
78.041054	2939.999877	21.713255
78.633039	2953.968840	21.718272
78.334925	2954.537512	21.723290
78.331257	2964.104737	21.728307
78.480655	2954.720790	21.733325
78.677179	2973.478125	21.738343
78.986128	2987.963555	21.743360
79.300671	2989.665575	21.748378
79.343036	2985.478590	21.753395
79.683082	2985.391832	21.758413
79.483849	2988.646798	21.763431
79.569842	2985.678532	21.768448
79.762611	2981.731249	21.773466
79.741626	2987.705452	21.778483
79.974578	2981.900826	21.783501
79.678181	2984.968707	21.788519
79.792025	2979.683741	21.793536
79.697327	2976.104027	21.798554
79.657541	2981.051068	21.803571
79.672441	2977.639455	21.808589
79.781534	2988.485639	21.813607
80.113510	2998.872578	21.818624
80.178433	3015.386458	21.823642
80.176352	3003.245745	21.828659
80.354302	3008.991029	21.833677
80.476003	3008.872244	21.838695
80.850791	3015.971949	21.843712
81.109691	3026.530424	21.848730
81.107549	3032.189340	21.853747
81.146012	3023.227603	21.858765
80.947646	3025.804903	21.863783
81.347772	3016.849938	21.868800
81.420217	3018.935260	21.873818
80.706304	3033.557085	21.878835
80.903067	3018.454886	21.883853
80.978408	3035.934348	21.888871
81.193985	3034.283579	21.893888
81.795585	3024.287878	21.898906
81.346644	3034.820816	21.903923
81.561952	3045.222734	21.908941
81.892785	3047.457481	21.913959
81.925486	3051.692988	21.918976
82.130574	3049.345554	21.923994
81.682973	3055.930024	21.929011
81.860027	3050.272792	21.934029
81.830160	3052.156138	21.939047
82.022899	3059.266263	21.944064
82.214869	3071.529461	21.949082
81.599134	3084.316284	21.954099
82.202975	3073.321008	21.959117
82.207288	3084.994385	21.964135
82.233316	3098.861343	21.969152
82.704141	3108.022700	21.974170
82.586254	3113.091740	21.979187
83.222166	3103.122994	21.984205
82.932472	3107.353921	21.989223
82.787115	3110.652369	21.994240
83.057925	3105.882346	21.999258
82.882386	3108.646432	22.004275
83.505803	3109.633670	22.009293
83.742851	3126.346382	22.014311
83.786377	3121.359986	22.019328
84.040484	3109.514244	22.024346
83.916484	3104.541757	22.029363
83.885588	3087.083895	22.034381
83.632968	3093.369635	22.039399
83.685828	3095.936926	22.044416
84.306144	3112.316614	22.049434
83.881200	3124.606605	22.054451
84.153935	3107.031618	22.059469
83.816708	3109.416139	22.064487
84.148246	3122.392900	22.069504
84.018976	3115.194198	22.074522
84.063015	3128.414923	22.079539
84.260619	3149.057264	22.084557
84.486005	3151.534640	22.089575
84.666923	3157.734984	22.094592
84.918169	3144.004714	22.099610
84.517794	3152.090028	22.104627
84.712176	3148.898315	22.109645
84.648837	3166.398873	22.114663
84.958693	3178.568268	22.119680
85.581900	3183.077084	22.124698
85.394479	3182.143661	22.129715
85.827660	3176.564921	22.134733
85.677867	3183.070311	22.139751
85.434945	3189.494246	22.144768
85.629518	3183.462429	22.149786
85.214184	3185.494527	22.154803
85.708507	3192.088749	22.159821
85.895491	3207.767336	22.164839
85.822277	3213.586090	22.169856
86.325195	3218.327779	22.174874
86.350491	3224.053094	22.179891
86.685644	3214.170592	22.184909
86.576461	3214.982846	22.189927
86.615555	3213.042729	22.194944
86.562259	3195.382941	22.199962
86.362275	3216.514682	22.204979
86.528842	3204.100675	22.209997
86.618453	3206.343417	22.215015
86.184484	3214.591790	22.220032
86.472660	3229.462363	22.225050
86.385391	3240.144329	22.230067
86.680243	3247.134913	22.235085
86.993845	3262.728067	22.240103
86.796393	3264.548190	22.245120
87.412945	3270.535256	22.250138
87.408830	3265.305118	22.255155
87.404554	3263.669003	22.260173
87.865395	3279.045328	22.265191
87.903397	3291.363277	22.270208
88.219960	3286.520680	22.275226
88.094328	3288.163980	22.280243
88.257060	3281.402761	22.285261
88.052195	3282.167052	22.290279
88.177092	3285.828741	22.295296
88.444173	3279.382554	22.300314
88.173307	3286.659943	22.305331
88.494226	3284.311444	22.310349
88.600767	3281.007058	22.315367
88.728320	3270.434829	22.320384
88.908921	3275.367591	22.325402
88.468425	3274.511416	22.330419
88.739571	3267.490561	22.335437
88.716524	3278.022180	22.340455
88.811045	3292.611044	22.345472
89.230157	3291.771082	22.350490
89.168823	3303.358230	22.355507
89.114171	3299.557262	22.360525
89.297233	3310.972144	22.365543
89.219956	3321.191108	22.370560
89.396156	3305.512513	22.375578
89.324603	3306.259500	22.380595
89.396402	3330.707819	22.385613
89.676134	3333.812843	22.390631
89.427476	3342.536554	22.395648
89.536787	3337.270720	22.400666
89.287909	3338.032051	22.405683
89.549829	3351.533489	22.410701
89.915886	3358.811170	22.415719
89.723853	3376.186383	22.420736
89.667766	3387.003058	22.425754
89.953909	3397.943497	22.430771
90.822130	3406.480319	22.435789
91.090311	3409.859703	22.440807
90.980345	3414.405888	22.445824
90.958440	3415.071055	22.450842
91.352455	3411.741184	22.455859
91.493587	3423.832750	22.460877
91.956024	3413.355082	22.465895
91.760616	3395.956341	22.470912
91.652395	3385.412760	22.475930
91.715401	3376.280231	22.480947
91.711949	3377.862801	22.485965
91.971950	3375.929858	22.490983
91.745157	3381.513822	22.496000
91.664191	3371.954309	22.501018
91.893420	3391.437441	22.506035
91.913461	3407.998526	22.511053
91.906858	3407.973381	22.516071
92.015583	3412.849168	22.521088
92.319864	3415.618268	22.526106
92.307714	3418.255017	22.531123
92.493319	3411.782870	22.536141
92.708246	3408.267637	22.541159
92.397849	3416.241763	22.546176
92.712053	3421.685949	22.551194
92.582177	3433.103815	22.556211
92.477879	3433.368038	22.561229
92.910399	3427.860971	22.566247
92.689253	3450.732325	22.571264
92.762314	3450.456224	22.576282
92.799906	3459.250807	22.581299
92.984383	3462.305851	22.586317
93.369022	3463.298321	22.591335
93.424435	3480.667800	22.596352
93.664257	3482.670016	22.601370
93.488272	3487.688936	22.606387
93.805640	3495.044018	22.611405
94.283392	3479.560690	22.616423
94.180407	3484.692741	22.621440
94.331661	3474.591254	22.626458
94.184524	3473.072818	22.631475
94.433763	3480.751351	22.636493
94.310186	3486.611599	22.641511
94.703250	3503.400905	22.646528
94.452567	3498.111828	22.651546
94.675831	3516.749657	22.656563
94.716371	3520.120227	22.661581
95.095678	3517.868737	22.666599
94.588123	3508.508765	22.671616
94.700447	3514.794996	22.676634
94.726089	3511.222831	22.681651
94.921659	3525.873169	22.686669
95.413834	3533.212374	22.691687
95.230606	3534.685299	22.696704
95.435011	3530.524146	22.701722
95.726745	3531.892206	22.706739
95.349335	3526.682328	22.711757
95.721410	3529.807959	22.716775
95.669344	3554.153084	22.721792
95.732156	3545.796465	22.726810
96.111394	3560.404280	22.731827
96.089361	3556.476600	22.736845
96.348823	3550.425258	22.741863
96.148546	3559.858019	22.746880
96.580571	3553.679341	22.751898
96.638292	3562.608450	22.756915
96.732812	3585.023117	22.761933
96.958960	3576.479650	22.766951
96.778527	3580.255643	22.771968
97.189179	3587.317010	22.776986
97.060213	3573.898795	22.782003
97.001692	3587.921105	22.787021
97.125428	3577.717800	22.792039
97.174082	3582.675221	22.797056
97.150151	3588.003296	22.802074
97.666571	3596.589698	22.807091
97.572412	3608.449819	22.812109
97.865349	3614.064123	22.817127
97.956343	3616.136225	22.822144
97.880553	3618.830374	22.827162
97.937916	3619.847410	22.832179
98.157185	3613.433396	22.837197
98.111690	3605.964323	22.842215
97.583403	3628.959921	22.847232
98.322205	3642.987926	22.852250
98.594297	3639.823036	22.857267
98.411419	3644.747871	22.862285
98.574436	3650.013972	22.867303
98.409899	3657.782623	22.872320
98.745413	3671.002889	22.877338
99.124046	3678.881004	22.882355
99.046189	3674.335354	22.887373
99.366887	3673.311243	22.892391
99.346330	3673.526592	22.897408
99.143938	3671.321205	22.902426
99.817973	3679.149325	22.907443
99.472065	3697.512529	22.912461
100.001095	3687.162650	22.917479
100.323183	3696.639095	22.922496
99.889090	3695.927505	22.927514
100.306987	3694.735755	22.932531
100.447779	3698.579168	22.937549
100.421352	3690.776588	22.942567
100.267698	3689.072593	22.947584
100.434805	3690.538427	22.952602
100.494803	3688.680229	22.957619
100.089963	3689.435459	22.962637
100.381392	3707.393356	22.967655
100.542823	3723.840862	22.972672
100.808510	3725.917970	22.977690
100.693547	3732.281219	22.982707
100.316972	3731.851461	22.987725
100.863865	3735.604154	22.992743
101.021663	3747.186918	22.997760
100.962522	3754.010638	23.002778
101.248525	3763.756867	23.007795
101.262976	3784.642133	23.012813
101.500373	3779.006556	23.017831
101.371269	3781.586314	23.022848
101.475834	3784.799117	23.027866
101.748419	3794.933412	23.032883
102.085418	3805.753926	23.037901
102.722045	3792.737753	23.042919
102.585734	3805.758935	23.047936
102.361806	3797.885788	23.052954
102.935964	3797.033959	23.057971
102.888457	3798.356134	23.062989
102.842607	3798.282355	23.068007
103.087743	3796.721506	23.073024
102.765537	3791.765803	23.078042
103.260980	3791.476198	23.083059
103.082042	3795.848851	23.088077
103.136711	3784.196971	23.093095
103.516240	3791.850980	23.098112
103.204716	3794.482538	23.103130
103.097829	3793.872385	23.108147
103.164016	3815.505448	23.113165
103.589697	3811.946243	23.118183
103.383316	3830.615289	23.123200
103.402610	3834.110306	23.128218
103.664621	3843.996772	23.133235
103.768998	3856.270736	23.138253
103.652864	3853.555787	23.143271
103.989697	3875.006019	23.148288
103.811295	3879.043562	23.153306
104.236706	3878.128514	23.158323
104.358250	3902.204941	23.163341
104.494974	3898.814727	23.168359
104.852661	3905.582626	23.173376
104.823695	3915.986126	23.178394
104.934818	3901.127541	23.183411
105.035865	3918.128546	23.188429
104.891032	3926.825190	23.193447
105.439797	3942.923092	23.198464
105.629893	3948.495061	23.203482
106.089657	3925.691704	23.208499
105.672936	3936.451030	23.213517
105.934682	3927.758179	23.218535
105.943835	3936.886870	23.223552
105.628720	3937.454052	23.228570
106.322993	3944.653758	23.233587
106.098649	3954.954134	23.238605
106.372691	3958.904728	23.243623
106.299158	3953.546457	23.248640
106.298469	3954.612085	23.253658
106.662288	3951.137088	23.258675
106.881966	3980.178606	23.263693
106.786544	3983.255203	23.268711
107.334618	3978.070588	23.273728
106.876933	3984.516951	23.278746
107.139280	3983.053635	23.283763
106.985896	3981.888943	23.288781
107.217451	3990.543112	23.293799
107.441037	4007.600739	23.298816
107.028555	4008.422206	23.303834
107.606731	4008.846108	23.308851
107.578659	4013.426573	23.313869
107.297639	4026.151372	23.318887
107.981902	4039.115500	23.323904
107.925311	4049.250812	23.328922
108.328043	4039.634187	23.333939
108.143450	4055.758114	23.338957
108.462842	4065.193891	23.343975
108.660204	4063.273185	23.348992
108.606460	4066.542915	23.354010
108.844108	4062.776926	23.359027
108.937138	4065.123562	23.364045
108.831361	4060.751708	23.369063
108.794121	4061.512352	23.374080
108.862626	4075.170795	23.379098
108.932409	4084.659248	23.384115
109.282995	4102.838542	23.389133
109.152442	4102.019684	23.394151
109.331174	4096.894094	23.399168
109.577020	4122.513355	23.404186
109.802740	4126.929864	23.409203
109.635067	4123.159182	23.414221
109.984251	4120.966917	23.419239
110.179186	4127.192501	23.424256
109.913912	4129.775525	23.429274
110.199999	4145.163086	23.434291
110.625639	4163.231620	23.439309
110.690409	4154.308980	23.444327
111.076709	4152.207431	23.449344
110.897947	4166.033196	23.454362
110.635227	4147.352176	23.459379
111.096421	4161.335580	23.464397
111.031849	4178.935121	23.469415
111.538662	4176.455376	23.474432
111.615957	4184.455595	23.479450
111.925912	4174.373889	23.484467
111.655305	4179.127949	23.489485
111.589256	4185.404163	23.494503
111.544553	4174.335360	23.499520
111.680281	4203.417152	23.504538
111.899879	4210.731643	23.509555
112.037264	4214.806463	23.514573
111.975945	4220.455904	23.519591
112.100887	4229.502246	23.524608
112.303258	4234.038396	23.529626
112.568667	4242.148903	23.534643
112.681903	4249.625875	23.539661
112.737573	4238.216413	23.544679
113.406098	4254.157837	23.549696
113.256328	4261.707804	23.554714
113.504670	4268.076986	23.559731
113.506893	4271.111912	23.564749
113.441137	4279.814978	23.569767
113.816871	4272.510633	23.574784
113.572164	4274.876495	23.579802
113.901332	4264.889197	23.584819
113.750243	4275.236343	23.589837
113.550040	4271.442652	23.594855
113.951092	4276.040082	23.599872
114.002119	4290.175242	23.604890
114.052644	4290.231998	23.609907
114.187410	4295.085255	23.614925
114.515877	4312.967650	23.619943
114.598789	4318.524000	23.624960
114.321946	4328.412020	23.629978
114.689227	4318.122315	23.634995
114.668764	4327.287626	23.640013
114.991303	4344.739918	23.645031
115.397847	4350.115629	23.650048
114.868612	4351.650530	23.655066
115.234022	4361.428898	23.660083
115.491361	4372.520069	23.665101
115.716510	4380.367211	23.670119
115.951119	4377.072141	23.675136
115.880802	4387.099701	23.680154
115.787960	4382.907910	23.685171
116.275640	4380.078524	23.690189
116.481857	4401.932186	23.695207
116.878403	4400.123414	23.700224
116.862446	4394.483417	23.705242
116.668818	4391.573690	23.710259
117.087515	4394.976454	23.715277
117.184080	4395.964227	23.720295
117.337486	4395.874449	23.725312
117.154459	4399.558937	23.730330
117.447731	4394.983640	23.735347
117.201553	4399.092362	23.740365
117.137682	4396.479711	23.745383
117.259615	4402.591085	23.750400
117.069022	4401.623856	23.755418
117.667587	4423.704461	23.760435
117.875443	4424.567936	23.765453
117.608011	4427.369092	23.770471
117.980642	4422.546804	23.775488
117.859163	4439.883590	23.780506
118.117201	4457.420686	23.785523
118.183631	4450.773305	23.790541
118.113858	4467.633051	23.795559
118.320238	4486.850454	23.800576
118.543151	4498.410025	23.805594
118.427609	4492.708098	23.810611
118.923099	4493.855166	23.815629
118.736969	4524.097886	23.820647
119.568512	4519.980486	23.825664
119.686166	4517.897690	23.830682
119.358403	4510.463408	23.835699
119.672220	4503.806229	23.840717
119.829510	4527.674557	23.845735
119.821660	4527.143290	23.850752
119.966474	4533.694265	23.855770
120.327694	4541.861148	23.860787
120.627069	4524.217169	23.865805
120.717868	4533.624072	23.870823
120.893987	4526.731749	23.875840
120.749918	4525.795016	23.880858
120.631050	4528.481478	23.885875
121.182376	4542.532621	23.890893
120.692064	4547.614452	23.895911
121.255959	4552.196080	23.900928
121.322609	4549.685070	23.905946
121.224421	4548.004493	23.910963
121.265331	4550.664162	23.915981
121.680583	4568.081306	23.920999
121.997242	4575.315360	23.926016
122.073368	4576.319121	23.931034
121.962298	4579.794112	23.936051
122.265399	4580.444995	23.941069
122.288245	4585.424718	23.946087
123.107614	4583.501959	23.951104
122.486112	4574.803905	23.956122
122.566040	4570.845340	23.961139
122.638315	4574.652653	23.966157
122.560273	4596.060618	23.971175
122.920916	4601.440065	23.976192
123.083200	4616.311118	23.981210
122.786209	4618.249818	23.986227
123.038830	4623.581370	23.991245
123.142899	4633.628306	23.996263
122.843621	4637.756495	24.001280
123.070194	4642.663592	24.006298
123.213452	4665.139482	24.011315
123.716680	4666.710115	24.016333
123.635615	4678.496441	24.021351
124.194795	4702.204525	24.026368
124.271956	4711.853176	24.031386
124.041200	4705.824517	24.036403
124.545097	4698.086959	24.041421
124.673361	4708.495717	24.046439
124.587975	4717.414489	24.051456
125.061321	4725.650742	24.056474
124.874170	4726.475956	24.061491
125.280116	4720.825577	24.066509
124.762996	4727.413175	24.071527
125.179118	4724.696347	24.076544
125.234779	4740.592291	24.081562
125.497076	4752.811731	24.086579
125.831854	4751.434021	24.091597
125.864895	4766.178926	24.096615
125.733645	4746.610834	24.101632
126.341603	4765.038158	24.106650
126.159790	4785.537876	24.111667
125.915080	4777.988947	24.116685
126.039040	4785.825848	24.121703
126.833589	4785.474995	24.126720
126.708397	4806.193353	24.131738
126.718037	4819.373165	24.136755
126.861507	4812.172703	24.141773
126.486314	4822.963177	24.146791
126.895216	4833.585506	24.151808
126.878428	4835.745666	24.156826
127.145541	4851.522129	24.161843
127.531351	4847.348371	24.166861
127.516472	4869.754617	24.171879
127.661094	4875.489170	24.176896
128.056285	4874.017997	24.181914
128.354318	4890.023660	24.186931
128.687572	4882.185854	24.191949
128.838848	4900.341137	24.196967
128.759595	4898.368000	24.201984
128.953743	4893.692394	24.207002
129.085462	4888.501081	24.212019
129.134724	4890.477880	24.217037
128.907177	4890.905416	24.222055
129.188648	4892.113868	24.227072
129.280432	4898.280422	24.232090
129.230476	4915.748841	24.237107
129.823165	4924.139115	24.242125
129.864082	4919.612060	24.247143
129.706520	4928.734626	24.252160
130.297080	4922.004373	24.257178
130.034385	4935.471430	24.262195
130.087552	4944.298533	24.267213
130.037870	4952.254375	24.272231
130.092573	4950.615424	24.277248
130.358343	4956.785537	24.282266
130.407141	4980.211818	24.287283
130.560393	4983.406194	24.292301
130.804639	4977.988759	24.297319
130.850632	5005.504068	24.302336
131.093153	5003.180084	24.307354
131.279688	5013.075831	24.312371
131.150203	5011.569680	24.317389
131.635050	5032.728918	24.322407
131.922464	5043.290750	24.327424
131.980696	5045.083394	24.332442
132.011985	5044.451933	24.337459
132.397859	5043.709119	24.342477
132.169347	5061.390292	24.347495
132.567022	5061.278654	24.352512
132.906341	5061.020345	24.357530
133.118417	5059.028578	24.362547
133.225109	5061.760938	24.367565
133.164541	5067.857056	24.372583
133.088762	5062.852742	24.377600
133.238785	5056.421626	24.382618
133.300073	5068.904077	24.387635
133.401091	5068.902488	24.392653
133.517098	5076.670764	24.397671
133.609761	5085.179188	24.402688
133.650405	5083.140542	24.407706
133.569796	5090.399928	24.412723
133.959751	5110.926075	24.417741
134.109945	5115.407714	24.422759
134.383321	5125.385254	24.427776
134.504357	5117.076841	24.432794
134.294026	5133.855797	24.437811
134.643434	5148.796839	24.442829
134.723235	5148.388876	24.447847
135.038109	5149.908393	24.452864
135.015269	5157.087391	24.457882
135.109441	5179.428418	24.462899
135.284125	5174.892966	24.467917
135.546909	5172.994391	24.472935
135.682654	5188.518467	24.477952
135.861269	5196.539475	24.482970
135.737613	5206.304694	24.487987
136.120492	5198.462074	24.493005
136.292371	5208.550149	24.498023
136.290833	5222.231014	24.503040
136.581270	5230.300891	24.508058
136.372545	5239.536827	24.513075
136.543033	5233.859812	24.518093
136.788485	5258.543512	24.523111
136.504185	5260.527047	24.528128
137.125016	5267.011879	24.533146
137.135960	5275.983955	24.538163
137.490882	5281.460657	24.543181
137.864775	5288.517066	24.548199
137.774153	5291.315144	24.553216
137.982283	5302.653718	24.558234
138.163393	5312.641505	24.563251
138.261076	5318.816308	24.568269
138.307437	5313.063702	24.573287
138.330623	5315.934720	24.578304
138.861079	5326.110091	24.583322
138.945738	5333.985261	24.588339
138.726673	5330.158203	24.593357
139.291439	5325.852769	24.598375
139.314022	5324.849074	24.603392
139.550745	5331.647431	24.608410
139.746262	5340.395718	24.613427
139.779829	5362.007966	24.618445
139.694233	5364.213037	24.623463
139.774885	5363.636012	24.628480
140.132230	5361.302452	24.633498
140.275525	5366.192434	24.638515
140.073240	5367.419830	24.643533
140.248768	5382.837122	24.648551
140.430766	5393.718613	24.653568
140.485792	5393.669893	24.658586
140.507140	5421.030146	24.663603
140.646973	5428.771035	24.668621
141.038337	5415.112480	24.673639
140.909726	5439.082206	24.678656
141.567733	5447.673413	24.683674
141.564108	5447.440269	24.688691
141.531046	5450.796645	24.693709
142.045874	5460.568735	24.698727
142.199282	5479.341732	24.703744
142.489444	5474.278393	24.708762
142.447361	5487.153105	24.713779
142.666335	5478.080593	24.718797
143.019828	5473.293436	24.723815
143.047238	5479.182242	24.728832
142.987480	5462.661239	24.733850
143.067680	5476.816278	24.738867
143.062708	5477.827199	24.743885
143.578615	5464.905195	24.748903
143.373380	5482.087664	24.753920
143.698146	5505.348644	24.758938
143.468495	5508.295339	24.763955
143.673822	5513.677144	24.768973
143.920582	5500.967714	24.773991
143.507446	5516.527296	24.779008
143.847040	5529.291725	24.784026
144.092725	5532.733963	24.789043
143.778931	5563.267534	24.794061
143.984700	5566.863637	24.799079
144.301456	5578.323848	24.804096
145.007987	5590.974932	24.809114
145.238498	5603.207379	24.814131
144.850204	5593.889040	24.819149
145.213720	5614.139476	24.824167
145.481947	5612.155687	24.829184
145.576430	5618.237818	24.834202
145.488343	5636.499659	24.839219
145.865174	5646.471856	24.844237
146.125821	5656.453809	24.849255
146.131940	5654.065631	24.854272
146.518874	5656.074931	24.859290
146.373247	5679.648179	24.864307
146.692074	5689.892228	24.869325
147.142423	5677.849891	24.874343
146.955074	5682.607182	24.879360
147.162239	5697.499805	24.884378
147.373765	5714.243143	24.889395
147.515929	5714.951384	24.894413
147.868841	5709.305086	24.899431
147.457947	5720.495037	24.904448
147.704961	5722.888930	24.909466
147.965228	5738.239020	24.914483
148.112662	5729.687306	24.919501
148.501378	5734.269492	24.924519
148.546714	5762.950173	24.929536
148.667796	5764.161967	24.934554
148.964275	5757.842996	24.939571
148.866961	5776.677466	24.944589
149.165108	5769.906974	24.949607
149.042631	5795.266966	24.954624
149.142571	5788.932815	24.959642
149.366414	5800.744808	24.964659
149.329251	5825.473740	24.969677
149.671202	5831.333147	24.974695
149.866204	5844.071719	24.979712
149.627696	5832.017877	24.984730
149.925513	5846.975595	24.989747
150.230299	5865.259411	24.994765
150.566988	5862.017648	24.999783
150.729270	5882.200094	25.004800
151.049221	5892.511028	25.009818
150.941266	5885.014566	25.014835
151.041456	5892.507869	25.019853
151.300049	5901.304718	25.024871
151.605498	5919.385702	25.029888
151.657268	5917.573883	25.034906
151.677501	5926.038819	25.039923
151.762099	5941.357102	25.044941
151.993236	5949.783264	25.049959
152.229496	5955.712946	25.054976
152.106938	5947.678237	25.059994
151.910335	5969.641213	25.065011
152.301657	5981.140981	25.070029
152.739660	5980.484409	25.075047
152.892988	5985.510349	25.080064
152.812424	5998.593444	25.085082
153.077061	6013.080355	25.090099
153.491406	6017.151229	25.095117
153.532995	6020.871037	25.100135
153.961438	6035.661661	25.105152
154.052313	6029.342692	25.110170
154.399910	6033.524614	25.115187
154.190718	6043.276530	25.120205
154.592438	6029.134164	25.125223
154.469971	6035.323182	25.130240
154.632832	6063.093519	25.135258
154.680187	6066.535966	25.140275
154.627145	6072.869457	25.145293
154.999772	6071.847250	25.150311
155.200597	6079.762664	25.155328
155.199864	6090.630732	25.160346
155.372750	6085.657454	25.165363
155.260798	6118.206307	25.170381
155.443224	6121.442167	25.175399
155.541868	6136.548839	25.180416
155.655309	6153.336023	25.185434
155.757215	6163.022431	25.190451
155.899845	6182.027221	25.195469
156.397753	6185.423596	25.200487
156.343315	6205.202828	25.205504
156.591237	6219.647803	25.210522
156.820981	6225.726721	25.215539
157.091266	6253.689914	25.220557
157.489059	6257.318632	25.225575
157.929731	6255.513389	25.230592
157.774661	6255.075299	25.235610
158.422423	6270.193743	25.240627
158.258712	6281.570843	25.245645
158.380370	6285.433416	25.250663
158.245109	6278.602016	25.255680
158.609407	6280.795091	25.260698
158.857485	6297.244381	25.265715
158.908993	6297.586463	25.270733
159.258361	6309.634835	25.275751
159.376908	6309.752419	25.280768
159.332319	6317.161169	25.285786
159.633437	6323.792993	25.290803
159.651223	6335.169280	25.295821
159.817844	6335.865634	25.300839
160.015557	6345.792273	25.305856
160.045796	6360.964804	25.310874
160.360171	6361.557203	25.315891
160.243479	6379.417478	25.320909
160.584506	6383.200512	25.325927
160.384094	6404.056264	25.330944
160.757459	6402.415697	25.335962
161.258953	6416.359819	25.340979
161.211984	6442.856611	25.345997
161.578608	6429.085892	25.351015
161.503876	6430.933350	25.356032
161.468222	6443.158850	25.361050
162.094025	6454.381991	25.366067
161.944935	6459.081610	25.371085
162.096229	6456.190103	25.376103
162.062951	6478.062615	25.381120
162.430499	6495.614620	25.386138
162.918368	6481.690727	25.391155
162.823188	6498.718301	25.396173
163.086236	6520.424563	25.401191
163.338279	6519.863279	25.406208
163.469277	6517.240517	25.411226
163.765098	6515.787587	25.416243
163.329456	6517.651375	25.421261
163.751045	6529.459595	25.426279
163.679845	6553.884610	25.431296
163.796358	6552.779474	25.436314
164.138464	6569.941205	25.441331
164.313605	6575.451222	25.446349
164.356392	6569.379398	25.451367
164.683036	6594.966522	25.456384
164.840225	6603.098112	25.461402
165.075397	6604.799088	25.466419
164.983601	6612.866292	25.471437
165.234744	6625.961251	25.476455
165.423077	6638.300314	25.481472
165.364348	6648.617616	25.486490
165.806281	6667.436504	25.491507
166.066730	6672.181135	25.496525
166.179435	6675.410516	25.501543
166.395333	6698.017899	25.506560
166.760587	6698.631045	25.511578
167.173974	6693.990348	25.516595
167.062140	6711.665909	25.521613
167.360479	6718.379478	25.526631
167.618486	6726.029027	25.531648
167.643448	6738.666083	25.536666
167.863079	6729.443895	25.541683
167.729684	6739.725554	25.546701
168.192070	6752.944012	25.551719
168.129610	6759.654212	25.556736
168.093401	6765.217332	25.561754
168.230257	6770.322639	25.566771
168.457033	6791.936038	25.571789
168.715856	6794.680579	25.576807
169.061320	6799.588402	25.581824
169.113848	6809.881913	25.586842
169.646989	6815.979445	25.591859
169.638987	6812.800747	25.596877
169.746838	6817.962053	25.601895
169.842099	6832.463533	25.606912
169.807794	6836.577255	25.611930
170.128158	6847.436105	25.616947
170.202326	6858.462441	25.621965
170.868590	6871.637861	25.626983
170.939331	6875.248309	25.632000
170.694939	6875.892893	25.637018
171.094189	6891.408981	25.642035
171.188383	6910.561266	25.647053
171.267823	6909.768594	25.652071
171.686796	6904.024325	25.657088
171.554506	6936.888530	25.662106
171.882890	6919.959269	25.667123
172.060146	6939.994114	25.672141
172.330849	6960.022206	25.677159
172.565097	6957.552425	25.682176
172.625882	6967.948634	25.687194
172.695652	6963.773384	25.692212
173.040447	6986.466205	25.697229
173.071578	6992.790094	25.702247
173.256208	6989.204648	25.707264
173.252207	7003.906191	25.712282
173.561777	7018.359830	25.717300
173.762696	7021.221088	25.722317
173.980227	7034.665322	25.727335
174.146147	7038.041924	25.732352
174.490893	7044.692835	25.737370
174.578756	7048.060285	25.742388
174.835976	7035.849968	25.747405
174.852846	7040.157691	25.752423
175.182705	7060.747913	25.757440
174.858387	7069.473590	25.762458
175.170072	7068.756733	25.767476
175.343050	7081.232568	25.772493
175.509299	7097.200834	25.777511
175.839686	7096.561218	25.782528
175.702338	7108.194456	25.787546
176.090738	7111.596531	25.792564
176.057428	7126.970893	25.797581
176.287157	7146.839028	25.802599
176.572088	7143.246426	25.807616
176.237563	7162.645486	25.812634
176.780413	7173.539469	25.817652
176.958997	7188.059012	25.822669
177.116161	7202.949906	25.827687
177.091260	7216.438292	25.832704
176.959087	7228.048711	25.837722
177.688557	7247.019253	25.842740
177.675537	7263.574917	25.847757
177.712896	7283.767203	25.852775
178.634163	7292.915678	25.857792
178.866964	7295.366114	25.862810
178.865801	7303.214711	25.867828
179.500573	7319.624017	25.872845
179.541933	7313.963260	25.877863
179.505963	7318.520791	25.882880
179.551885	7325.103060	25.887898
179.636068	7341.234776	25.892916
180.183588	7350.337142	25.897933
180.024409	7342.046686	25.902951
180.150731	7351.476190	25.907968
180.552604	7377.101775	25.912986
180.989913	7376.971376	25.918004
181.002089	7382.007699	25.923021
180.931382	7403.441905	25.928039
181.300515	7404.291505	25.933056
181.511310	7409.281629	25.938074
181.525035	7415.482550	25.943092
181.677377	7426.992547	25.948109
181.781953	7446.545439	25.953127
182.087940	7442.349934	25.958144
182.252792	7467.469818	25.963162
182.047383	7464.413392	25.968180
182.674702	7487.027173	25.973197
182.943085	7514.747982	25.978215
183.041892	7497.389783	25.983232
183.070709	7510.735653	25.988250
183.257192	7521.598190	25.993268
183.861887	7510.975375	25.998285
183.182549	7529.540304	26.003303
183.817284	7545.713574	26.008320
183.439067	7554.509068	26.013338
183.877580	7580.021816	26.018356
184.592551	7580.621320	26.023373
184.314280	7599.684768	26.028391
184.945512	7614.465427	26.033408
185.043645	7626.545298	26.038426
185.141321	7632.613505	26.043444
185.428007	7636.280595	26.048461
185.698322	7655.174705	26.053479
185.874831	7643.482108	26.058496
185.823286	7659.665717	26.063514
185.932866	7675.473023	26.068532
186.281646	7678.283192	26.073549
186.638856	7699.131213	26.078567
186.697847	7700.280171	26.083584
186.988606	7717.254739	26.088602
187.054932	7715.593104	26.093620
187.886401	7721.678717	26.098637
187.497957	7733.346027	26.103655
187.812209	7739.789620	26.108672
187.796992	7746.424697	26.113690
187.840030	7744.609386	26.118708
188.138664	7754.603726	26.123725
188.226555	7779.012225	26.128743
188.342050	7768.459833	26.133760
188.312170	7787.094174	26.138778
188.358189	7814.126077	26.143796
188.854746	7811.734115	26.148813
188.997778	7834.806469	26.153831
189.356861	7844.364781	26.158848
188.981079	7858.552806	26.163866
189.368898	7876.929996	26.168884
189.801916	7889.243786	26.173901
189.622300	7908.072347	26.178919
189.893071	7931.235575	26.183936
190.397862	7945.589286	26.188954
190.587630	7958.990065	26.193972
191.029648	7972.198740	26.198989
190.794291	7983.054110	26.204007
191.173062	7996.471735	26.209024
191.722897	8011.863232	26.214042
191.375579	8011.489935	26.219060
192.102874	8027.307368	26.224077
191.666360	8041.714311	26.229095
192.023353	8050.776106	26.234112
192.733990	8065.338500	26.239130
192.454314	8071.664557	26.244148
192.569474	8083.972737	26.249165
192.520863	8104.967111	26.254183
193.533766	8105.340985	26.259200
193.686313	8126.454948	26.264218
194.031081	8143.510840	26.269236
194.299179	8138.807882	26.274253
194.014534	8155.851218	26.279271
194.335189	8162.669624	26.284288
194.646508	8163.200381	26.289306
194.875593	8185.362708	26.294324
195.181839	8179.694106	26.299341
195.149413	8195.001624	26.304359
195.788174	8198.438183	26.309376
195.478971	8215.491942	26.314394
195.570666	8216.743439	26.319412
196.095093	8222.442848	26.324429
195.993427	8246.398209	26.329447
196.459140	8249.747591	26.334464
196.479963	8251.900823	26.339482
196.799220	8273.456077	26.344500
196.779876	8274.848797	26.349517
197.006152	8281.157498	26.354535
196.908644	8297.374557	26.359552
197.320248	8319.174533	26.364570
197.389436	8324.356112	26.369588
197.568350	8336.496427	26.374605
198.077421	8349.988127	26.379623
197.923055	8373.490046	26.384640
198.260390	8374.044080	26.389658
198.263316	8383.680471	26.394676
198.884418	8390.424128	26.399693
198.686711	8404.083853	26.404711
199.051049	8430.775936	26.409728
199.483439	8433.222716	26.414746
199.359523	8445.867620	26.419764
199.940223	8462.748611	26.424781
199.468653	8476.759254	26.429799
200.112577	8476.709709	26.434816
200.350691	8491.271023	26.439834
200.278038	8507.502305	26.444852
200.989384	8509.550141	26.449869
200.687457	8517.160758	26.454887
201.166329	8514.322660	26.459904
201.347706	8531.516238	26.464922
201.255937	8545.101082	26.469940
201.700623	8554.151040	26.474957
201.713604	8564.675920	26.479975
202.089779	8576.316751	26.484992
201.930983	8584.974950	26.490010
202.499052	8608.873756	26.495028
203.014754	8621.919573	26.500045
202.981689	8628.454787	26.505063
203.302108	8637.892370	26.510080
203.534626	8638.907968	26.515098
203.645563	8648.048570	26.520116
203.797594	8649.524852	26.525133
204.013250	8666.352169	26.530151
203.744318	8683.829832	26.535168
203.941224	8692.985399	26.540186
204.406758	8711.487770	26.545204
204.547073	8731.515237	26.550221
204.883797	8743.232024	26.555239
205.070274	8757.814717	26.560256
205.754448	8770.888744	26.565274
205.260296	8773.113747	26.570292
206.011036	8784.632980	26.575309
206.403004	8792.795433	26.580327
206.489400	8800.646846	26.585344
206.751688	8808.289613	26.590362
207.174790	8822.764743	26.595380
207.292130	8833.063827	26.600397
207.055380	8839.928942	26.605415
207.155421	8839.878685	26.610432
207.896242	8855.904235	26.615450
207.633819	8874.845293	26.620468
207.677407	8878.111753	26.625485
208.146352	8896.090769	26.630503
208.254303	8898.106818	26.635520
208.547102	8908.696751	26.640538
208.593480	8932.321497	26.645556
208.982758	8944.570087	26.650573
209.202257	8959.735108	26.655591
209.038178	8973.354320	26.660608
209.722043	8983.569347	26.665626
209.474012	9002.254550	26.670644
209.898494	9011.135610	26.675661
210.281620	9017.702250	26.680679
210.252065	9029.295455	26.685696
210.516112	9044.340559	26.690714
210.427368	9058.762635	26.695732
211.004791	9070.290236	26.700749
211.220841	9083.023617	26.705767
211.639526	9097.661988	26.710784
212.012158	9112.630928	26.715802
211.804877	9127.043508	26.720820
212.155783	9128.472009	26.725837
212.179507	9138.366930	26.730855
212.326552	9161.139660	26.735872
212.807748	9157.225102	26.740890
212.604587	9175.771553	26.745908
213.139355	9195.581620	26.750925
213.437530	9205.383975	26.755943
213.241934	9220.608379	26.760960
213.723931	9237.357636	26.765978
213.716042	9244.859363	26.770996
214.437815	9252.590263	26.776013
214.423847	9269.304138	26.781031
214.365309	9275.315292	26.786048
214.940187	9282.738076	26.791066
214.836622	9306.362158	26.796084
215.122458	9315.705825	26.801101
215.211269	9326.291146	26.806119
215.485694	9340.154079	26.811136
215.782251	9351.136742	26.816154
215.594978	9370.670913	26.821172
215.941052	9386.297491	26.826189
216.296098	9397.591898	26.831207
216.462334	9418.275242	26.836224
216.741238	9439.722960	26.841242
216.756262	9457.373530	26.846260
217.233023	9464.508563	26.851277
217.773075	9465.159902	26.856295
217.576916	9504.699903	26.861312
218.136067	9507.388999	26.866330
218.195253	9521.034016	26.871348
218.490201	9526.639486	26.876365
219.004074	9532.634928	26.881383
219.189352	9551.772207	26.886400
219.625751	9548.864542	26.891418
219.594478	9555.873245	26.896436
219.715956	9559.757131	26.901453
219.826303	9586.732585	26.906471
219.882067	9584.647145	26.911488
220.470515	9593.251742	26.916506
220.764686	9620.637204	26.921524
220.414801	9625.177946	26.926541
221.152218	9633.837509	26.931559
220.929386	9648.964420	26.936576
221.467200	9658.772359	26.941594
221.589101	9677.983278	26.946612
222.172879	9683.295318	26.951629
222.329438	9690.708643	26.956647
222.258835	9719.308528	26.961664
222.848227	9719.949363	26.966682
222.714803	9735.639758	26.971700
222.975112	9749.672374	26.976717
222.980314	9756.180459	26.981735
223.041497	9792.188333	26.986752
223.412315	9787.593167	26.991770
223.585156	9805.784408	26.996788
224.006617	9829.199633	27.001805
224.139105	9830.296429	27.006823
224.297212	9854.528734	27.011840
224.561714	9864.767938	27.016858
225.083206	9873.138772	27.021876
225.181594	9897.802436	27.026893
225.406618	9901.917426	27.031911
225.610883	9928.064234	27.036928
226.055531	9932.321755	27.041946
226.232721	9938.978734	27.046964
226.152596	9964.759828	27.051981
226.980059	9966.834367	27.056999
226.970636	9978.736870	27.062016
227.358938	10000.354745	27.067034
227.260787	10004.907565	27.072052
227.548073	10013.524341	27.077069
228.034690	10030.681711	27.082087
227.581239	10032.608701	27.087104
227.946443	10045.156727	27.092122
228.241430	10057.595843	27.097140
228.864999	10069.874336	27.102157
228.886389	10087.940469	27.107175
228.971139	10097.825902	27.112192
229.006423	10094.042301	27.117210
229.031157	10108.000725	27.122228
229.350119	10127.226888	27.127245
229.559219	10143.822111	27.132263
229.919212	10151.178406	27.137280
230.329550	10179.655539	27.142298
230.319189	10194.575347	27.147316
230.715744	10205.775247	27.152333
230.938843	10211.859166	27.157351
230.973749	10231.802745	27.162368
231.365306	10247.703874	27.167386
231.540136	10264.492365	27.172404
231.576203	10291.457652	27.177421
231.873406	10305.019900	27.182439
231.993082	10319.151876	27.187456
232.368170	10333.664677	27.192474
232.998823	10360.302609	27.197492
233.122454	10366.367574	27.202509
233.760014	10384.141601	27.207527
233.656664	10401.835619	27.212544
234.059971	10398.825352	27.217562
234.547639	10405.319368	27.222580
234.577191	10414.533513	27.227597
235.243046	10420.262347	27.232615
235.435034	10428.784023	27.237632
235.674164	10435.498721	27.242650
235.767240	10438.522578	27.247668
235.881287	10442.026643	27.252685
236.244822	10453.778076	27.257703
236.294115	10458.630424	27.262720
236.593695	10470.839085	27.267738
237.003284	10484.509743	27.272756
236.916038	10513.569113	27.277773
237.084787	10505.089690	27.282791
237.493403	10508.259937	27.287808
237.509180	10520.780996	27.292826
237.673928	10531.459341	27.297844
237.334613	10550.111018	27.302861
237.689394	10558.843765	27.307879
238.147962	10581.340969	27.312896
238.643079	10603.710853	27.317914
238.952107	10627.318345	27.322932
238.798080	10638.119540	27.327949
239.053366	10657.727106	27.332967
239.301540	10670.866868	27.337984
239.686986	10694.301131	27.343002
239.697272	10715.461730	27.348020
239.689944	10733.611324	27.353037
240.124822	10755.124057	27.358055
240.727970	10775.418719	27.363072
241.035804	10793.337488	27.368090
241.345141	10803.231152	27.373108
241.329686	10822.675686	27.378125
241.742845	10834.308127	27.383143
241.941337	10852.947708	27.388160
242.129060	10866.186635	27.393178
242.354426	10879.238957	27.398196
242.377869	10903.620357	27.403213
242.850481	10911.245931	27.408231
243.060346	10929.423670	27.413248
243.302513	10953.907654	27.418266
243.509972	10965.671072	27.423284
243.572453	10985.516502	27.428301
243.829747	11005.287230	27.433319
243.885236	11022.152953	27.438336
244.385101	11038.154354	27.443354
244.720994	11061.795861	27.448372
244.822754	11069.875093	27.453389
245.061434	11090.385566	27.458407
245.166908	11108.965188	27.463424
245.323230	11116.292561	27.468442
245.859990	11133.408172	27.473460
246.046988	11160.687152	27.478477
246.115525	11167.527240	27.483495
246.264273	11192.718690	27.488512
246.406588	11209.773511	27.493530
247.133890	11224.993860	27.498548
246.772374	11251.544333	27.503565
247.218179	11265.314452	27.508583
247.859160	11293.478163	27.513600
247.880752	11316.514179	27.518618
248.286480	11329.210926	27.523636
248.325774	11354.329332	27.528653
248.688357	11367.405859	27.533671
248.866690	11388.656172	27.538688
249.285887	11416.400616	27.543706
249.826715	11423.858396	27.548724
250.039669	11442.319809	27.553741
250.584738	11453.735536	27.558759
250.675654	11464.038322	27.563776
250.897959	11475.677555	27.568794
251.343402	11498.795846	27.573812
251.358450	11504.919361	27.578829
251.611791	11525.268834	27.583847
251.806267	11536.599168	27.588864
251.969934	11553.249053	27.593882
252.371651	11570.441015	27.598900
252.404422	11582.927795	27.603917
253.060916	11594.645846	27.608935
252.841109	11619.179602	27.613952
253.016962	11637.647370	27.618970
253.392448	11647.797692	27.623988
253.485988	11675.206430	27.629005
253.968491	11690.091889	27.634023
254.021843	11705.410657	27.639040
254.224966	11733.345758	27.644058
254.636602	11746.537388	27.649076
254.805332	11772.927846	27.654093
255.629630	11794.706938	27.659111
255.658352	11805.665432	27.664128
255.334105	11823.948976	27.669146
256.000926	11839.201963	27.674164
255.918050	11866.897788	27.679181
256.500492	11887.512408	27.684199
256.798731	11909.156410	27.689216
256.615909	11926.831361	27.694234
257.309522	11939.025672	27.699252
257.402296	11969.195531	27.704269
257.524400	11986.227730	27.709287
257.935330	12013.596422	27.714304
258.117128	12031.849374	27.719322
258.669568	12046.990681	27.724340
258.502570	12066.717797	27.729357
258.777800	12084.901802	27.734375
259.477220	12114.981156	27.739392
259.302276	12130.616936	27.744410
259.763864	12147.833501	27.749428
259.947420	12173.327988	27.754445
260.531107	12182.496498	27.759463
260.883494	12209.625455	27.764480
261.164552	12228.408194	27.769498
261.671174	12232.177101	27.774516
261.697214	12259.976144	27.779533
262.000559	12258.886233	27.784551
262.321257	12274.145614	27.789568
262.364307	12292.462754	27.794586
262.413520	12292.338165	27.799604
262.648262	12322.211065	27.804621
262.858298	12328.669018	27.809639
263.057268	12356.527104	27.814656
263.005822	12375.884134	27.819674
263.545717	12386.422161	27.824692
263.768545	12415.183203	27.829709
263.783079	12429.434465	27.834727
264.321137	12453.618953	27.839744
264.439352	12477.190575	27.844762
265.019780	12497.390333	27.849780
265.064824	12523.388052	27.854797
265.663825	12529.024706	27.859815
266.315243	12544.681135	27.864832
266.208517	12559.318105	27.869850
266.451423	12574.432267	27.874868
266.910924	12596.439745	27.879885
267.022481	12608.540078	27.884903
267.501872	12623.252018	27.889920
267.508893	12653.198607	27.894938
268.048042	12650.995089	27.899956
268.147628	12672.929779	27.904973
268.373400	12687.020312	27.909991
268.855876	12699.298935	27.915008
268.794976	12721.000216	27.920026
269.062918	12732.844752	27.925044
269.306880	12764.573911	27.930061
269.474652	12778.864768	27.935079
269.643301	12794.382968	27.940096
269.871203	12817.226321	27.945114
270.281671	12837.359257	27.950132
270.743726	12856.788804	27.955149
271.107977	12883.225986	27.960167
271.610285	12898.528437	27.965184
271.683439	12927.935168	27.970202
272.242219	12922.838500	27.975220
272.317169	12944.733509	27.980237
272.675786	12955.116714	27.985255
273.482778	12972.749813	27.990272
273.548174	12976.380651	27.995290
273.825198	12984.059230	28.000308
274.045917	13018.115348	28.005325
273.998721	13015.696665	28.010343
274.088757	13034.220394	28.015360
274.229423	13058.124786	28.020378
274.938374	13074.664880	28.025396
275.049532	13090.413466	28.030413
275.487004	13098.878671	28.035431
275.696204	13115.253984	28.040448
275.699460	13147.872990	28.045466
276.149063	13146.265651	28.050484
276.687118	13164.926658	28.055501
276.795138	13190.703897	28.060519
276.743334	13201.972883	28.065536
277.175612	13214.641526	28.070554
277.785845	13229.360766	28.075572
277.735330	13245.385184	28.080589
277.839397	13268.208665	28.085607
278.146751	13275.622373	28.090624
278.105579	13308.636678	28.095642
278.579612	13320.493293	28.100660
279.144334	13336.137242	28.105677
279.132623	13365.719518	28.110695
279.567740	13380.485163	28.115712
279.623786	13400.521358	28.120730
280.035089	13418.946752	28.125748
280.545415	13446.898672	28.130765
280.608633	13451.437621	28.135783
281.377198	13474.644822	28.140800
281.073871	13495.180151	28.145818
281.465780	13504.343287	28.150836
282.005824	13528.483363	28.155853
281.674488	13556.314528	28.160871
282.069585	13566.080697	28.165888
281.999091	13595.603770	28.170906
282.368314	13607.198998	28.175924
282.805348	13634.566129	28.180941
282.834753	13659.989944	28.185959
283.372882	13668.670461	28.190976
283.673770	13714.328394	28.195994
284.063662	13734.703795	28.201012
284.159671	13747.701027	28.206029
284.228382	13777.141550	28.211047
284.685080	13801.076767	28.216064
284.974348	13826.010379	28.221082
285.188296	13851.344123	28.226100
286.110163	13879.819727	28.231117
286.086468	13906.157218	28.236135
286.924666	13925.645670	28.241152
286.925006	13932.338253	28.246170
286.981387	13954.267635	28.251188
287.207946	13975.670971	28.256205
287.471294	14000.114325	28.261223
288.000046	14032.927210	28.266240
288.154545	14050.269034	28.271258
288.487960	14067.582893	28.276276
288.984663	14099.764573	28.281293
289.031107	14116.785516	28.286311
289.817308	14121.958453	28.291328
290.432477	14139.972786	28.296346
290.740616	14154.380340	28.301364
291.053181	14157.929635	28.306381
291.017832	14185.632606	28.311399
291.634376	14199.492856	28.316416
291.759058	14211.702529	28.321434
291.870249	14238.601335	28.326452
292.397753	14241.221631	28.331469
292.529652	14260.546680	28.336487
292.631328	14284.612181	28.341504
292.611316	14296.743393	28.346522
292.176626	14310.229023	28.351540
292.832733	14341.462971	28.356557
293.230224	14371.124450	28.361575
293.960483	14399.111016	28.366592
293.798361	14421.143315	28.371610
294.328540	14451.028852	28.376628
294.652231	14471.435027	28.381645
294.762995	14499.943300	28.386663
295.062642	14522.917458	28.391680
295.439267	14544.747451	28.396698
295.782714	14569.885999	28.401716
295.936366	14593.792085	28.406733
296.025064	14622.190754	28.411751
296.711153	14643.643543	28.416768
297.121896	14673.686325	28.421786
297.122414	14698.637466	28.426804
297.782043	14710.669306	28.431821
297.711643	14746.912487	28.436839
298.286890	14759.968455	28.441856
298.554263	14788.243340	28.446874
299.127136	14808.734842	28.451892
299.277640	14838.534110	28.456909
299.561142	14854.835869	28.461927
299.757023	14870.193967	28.466944
300.160787	14889.418114	28.471962
300.421814	14895.046834	28.476980
300.546120	14917.740065	28.481997
300.511113	14939.810370	28.487015
301.134494	14952.313274	28.492032
301.459205	14987.966933	28.497050
301.382787	15010.643026	28.502068
301.817747	15030.208888	28.507085
302.338791	15061.515390	28.512103
302.644725	15079.299767	28.517120
303.044651	15116.009759	28.522138
302.979015	15132.412029	28.527156
303.315271	15156.490491	28.532173
303.812907	15187.969729	28.537191
304.014252	15205.760492	28.542208
304.078842	15244.655273	28.547226
304.358867	15273.586078	28.552244
304.822165	15286.330017	28.557261
305.099261	15321.297278	28.562279
305.521164	15344.687360	28.567296
305.606499	15376.113731	28.572314
306.092693	15407.527517	28.577332
306.569742	15434.906831	28.582349
306.447621	15454.941896	28.587367
306.879084	15478.708824	28.592384
307.219924	15509.752829	28.597402
307.554940	15537.480431	28.602420
308.407481	15556.172613	28.607437
308.471417	15584.559712	28.612455
308.832084	15605.216508	28.617472
309.016938	15624.680992	28.622490
309.402235	15666.968888	28.627508
309.764224	15676.040488	28.632525
309.859083	15709.016696	28.637543
310.368231	15740.335923	28.642560
310.748898	15760.729573	28.647578
311.050562	15790.757765	28.652596
311.266143	15813.511232	28.657613
311.326007	15839.924719	28.662631
311.741484	15865.568718	28.667648
312.034843	15877.192289	28.672666
312.544441	15915.668423	28.677684
313.390333	15940.001109	28.682701
313.684118	15965.200446	28.687719
313.933764	15994.975988	28.692736
314.062497	16001.392893	28.697754
314.179296	16029.565572	28.702772
314.587838	16050.393112	28.707789
314.876924	16061.787422	28.712807
315.287831	16098.363846	28.717824
315.960897	16100.692479	28.722842
316.158108	16133.236560	28.727860
316.682594	16133.520416	28.732877
316.497338	16160.539136	28.737895
317.289851	16177.914932	28.742912
317.680136	16195.900931	28.747930
317.762252	16214.323994	28.752948
317.963914	16227.189122	28.757965
318.144244	16242.500648	28.762983
318.648278	16254.132235	28.768000
319.008393	16287.641040	28.773018
319.472830	16300.320968	28.778036
319.611148	16314.747460	28.783053
319.694925	16347.430487	28.788071
320.287589	16352.746450	28.793088
320.456575	16381.894569	28.798106
320.484422	16409.535706	28.803124
320.769057	16440.631743	28.808141
320.862127	16464.188081	28.813159
321.172984	16485.590241	28.818176
321.345846	16505.831602	28.823194
321.568250	16537.760810	28.828212
321.875412	16554.537907	28.833229
322.131855	16587.933640	28.838247
322.237621	16620.851565	28.843264
322.862356	16647.404713	28.848282
323.139143	16675.221092	28.853300
323.799451	16701.082854	28.858317
323.841677	16742.405752	28.863335
324.177016	16758.834816	28.868352
324.874526	16788.725362	28.873370
325.149948	16818.137216	28.878388
325.606597	16842.322783	28.883405
325.972438	16866.063167	28.888423
326.222014	16891.501344	28.893440
326.873607	16917.804621	28.898458
327.074380	16937.305861	28.903476
327.764049	16955.769655	28.908493
328.160424	16979.905491	28.913511
328.421901	16992.430355	28.918528
328.944858	17013.780826	28.923546
329.032697	17039.039481	28.928564
329.196905	17038.536506	28.933581
329.396170	17068.476781	28.938599
329.564588	17093.868787	28.943616
330.059799	17111.411328	28.948634
330.308959	17141.962910	28.953652
330.380149	17164.649117	28.958669
330.882784	17192.036603	28.963687
331.054167	17222.684719	28.968704
331.276790	17250.468466	28.973722
331.566409	17284.268352	28.978740
332.034059	17305.075115	28.983757
332.355896	17336.236051	28.988775
332.666159	17369.276151	28.993792
333.287072	17392.256432	28.998810
333.123156	17431.332849	29.003828
333.811354	17456.538668	29.008845
334.230086	17489.003129	29.013863
334.160694	17513.476765	29.018880
334.991816	17537.032495	29.023898
335.048645	17578.605689	29.028916
335.456634	17598.752808	29.033933
335.925029	17628.512511	29.038951
336.223914	17657.873129	29.043968
336.505583	17674.335619	29.048986
336.871114	17713.282677	29.054004
337.087829	17743.479789	29.059021
337.502472	17766.174705	29.064039
337.730962	17798.505707	29.069056
338.211915	17819.154880	29.074074
338.353214	17863.602421	29.079092
338.838396	17874.172767	29.084109
339.348233	17903.790568	29.089127
339.571097	17932.506959	29.094144
340.222734	17950.357134	29.099162
340.290361	17988.835488	29.104180
340.770916	18018.089499	29.109197
340.983589	18046.429481	29.114215
341.626066	18073.694454	29.119232
341.978530	18094.590599	29.124250
341.893712	18129.491231	29.129268
342.348412	18158.300540	29.134285
342.873553	18176.572219	29.139303
342.731438	18218.875008	29.144320
343.305834	18231.544571	29.149338
343.380338	18268.873368	29.154356
343.377019	18291.017021	29.159373
343.775712	18315.854283	29.164391
344.013617	18352.149055	29.169408
344.646754	18381.119999	29.174426
345.142876	18423.239055	29.179444
345.292091	18449.790135	29.184461
345.483874	18482.150606	29.189479
345.672186	18522.326804	29.194496
346.208639	18543.927658	29.199514
346.684284	18580.967057	29.204532
346.975051	18620.103571	29.209549
347.532923	18650.001656	29.214567
347.990189	18681.820556	29.219584
348.387764	18708.368851	29.224602
348.811161	18739.416352	29.229620
349.287292	18762.469754	29.234637
349.971447	18794.866138	29.239655
350.146781	18819.400580	29.244672
350.844101	18820.830280	29.249690
350.872211	18855.436358	29.254708
351.369081	18869.126470	29.259725
351.650816	18889.043818	29.264743
351.511769	18926.209187	29.269760
352.051320	18944.424167	29.274778
352.377434	18980.511859	29.279796
352.783667	19005.783972	29.284813
353.485096	19018.899742	29.289831
353.131049	19067.513407	29.294848
353.797728	19083.588977	29.299866
353.852235	19122.783049	29.304884
354.258781	19157.812741	29.309901
354.560276	19174.643887	29.314919
354.748420	19219.566530	29.319936
355.366300	19251.424620	29.324954
355.971712	19289.074696	29.329972
356.285640	19328.300483	29.334989
356.797770	19338.868897	29.340007
357.232585	19384.928759	29.345024
357.716385	19397.199610	29.350042
357.613557	19424.703440	29.355060
358.090220	19450.506858	29.360077
358.490609	19481.619453	29.365095
358.571401	19514.068057	29.370112
359.287278	19542.883920	29.375130
359.309732	19577.274897	29.380148
359.976234	19617.466177	29.385165
360.627144	19639.418422	29.390183
360.282227	19678.971420	29.395200
361.136013	19707.063301	29.400218
361.327168	19739.926039	29.405236
361.329010	19762.083412	29.410253
361.789723	19788.738082	29.415271
362.407691	19832.650273	29.420288
362.777749	19850.769719	29.425306
363.352478	19886.212975	29.430324
363.350940	19925.635739	29.435341
364.049458	19945.948960	29.440359
364.219765	19981.002077	29.445376
364.426182	20002.411864	29.450394
365.007096	20029.933000	29.455412
365.025663	20067.497353	29.460429
365.795488	20100.112291	29.465447
365.720949	20135.086375	29.470464
366.277964	20167.342499	29.475482
366.536806	20202.969459	29.480500
366.623548	20243.190244	29.485517
367.263558	20271.152873	29.490535
367.535641	20320.918434	29.495552
367.910300	20356.055234	29.500570
368.330776	20369.235834	29.505588
368.656654	20406.374989	29.510605
369.487301	20430.918629	29.515623
369.605730	20464.362328	29.520640
369.792518	20496.506845	29.525658
370.661311	20528.464660	29.530676
370.673737	20556.001760	29.535693
370.526833	20574.847438	29.540711
371.131668	20610.424414	29.545728
371.693841	20632.975923	29.550746
372.381191	20661.475266	29.555764
372.769802	20695.147520	29.560781
373.288510	20710.850272	29.565799
373.404857	20745.694780	29.570816
373.795548	20780.374227	29.575834
374.362544	20805.542118	29.580852
374.306256	20844.020751	29.585869
375.090073	20862.055602	29.590887
375.078228	20897.440267	29.595904
375.419409	20934.106699	29.600922
375.838982	20961.151553	29.605940
376.141481	20994.581669	29.610957
376.885887	21028.235229	29.615975
376.720643	21058.239770	29.620992
377.443839	21095.587554	29.626010
377.694400	21130.525776	29.631028
377.760679	21170.758480	29.636045
378.587817	21204.846457	29.641063
378.946360	21244.944348	29.646080
379.149335	21273.836908	29.651098
379.802759	21311.117874	29.656116
379.860189	21339.028770	29.661133
380.250324	21386.241370	29.666151
380.975230	21416.706461	29.671168
381.557073	21441.631650	29.676186
382.031883	21475.945499	29.681204
382.496378	21506.070675	29.686221
383.031927	21526.192035	29.691239
383.522014	21560.377410	29.696256
383.781815	21589.004149	29.701274
384.488308	21604.719288	29.706292
384.315457	21635.531735	29.711309
384.577323	21660.711911	29.716327
385.098924	21698.619339	29.721344
385.257790	21733.624417	29.726362
385.700656	21757.379578	29.731380
385.883260	21792.538514	29.736397
386.316734	21822.855420	29.741415
386.142793	21866.025636	29.746432
386.549375	21897.133830	29.751450
387.242623	21929.099681	29.756468
387.803041	21975.494366	29.761485
388.076912	22013.178564	29.766503
388.174753	22055.304810	29.771520
388.671233	22103.164029	29.776538
389.506462	22135.147809	29.781556
389.523407	22181.733748	29.786573
389.902724	22218.204344	29.791591
390.299025	22257.391868	29.796608
390.665493	22300.068731	29.801626
391.194420	22330.583628	29.806644
391.224342	22378.445029	29.811661
391.612110	22404.515231	29.816679
392.255065	22455.657439	29.821696
392.770246	22495.180619	29.826714
393.415576	22523.232854	29.831732
393.529765	22562.012045	29.836749
393.826711	22574.341336	29.841767
394.432081	22620.110754	29.846784
394.629940	22648.475195	29.851802
394.929206	22682.705415	29.856820
395.406404	22724.649263	29.861837
395.942324	22750.347086	29.866855
396.360039	22801.866537	29.871872
396.621137	22827.920482	29.876890
397.109710	22860.629842	29.881908
397.488165	22903.389818	29.886925
397.663492	22934.254333	29.891943
398.317262	22962.813597	29.896960
398.597010	23004.570026	29.901978
399.173233	23028.837874	29.906996
398.991983	23076.830741	29.912013
399.687399	23107.992791	29.917031
400.173555	23146.295629	29.922048
400.440102	23193.194730	29.927066
400.983751	23214.399970	29.932084
401.104231	23259.481798	29.937101
401.545191	23299.459028	29.942119
402.409364	23338.198094	29.947136
402.722004	23393.744713	29.952154
403.264194	23416.054151	29.957172
403.549625	23468.713808	29.962189
404.072638	23501.861783	29.967207
404.140148	23534.817027	29.972224
403.979463	23572.584383	29.977242
405.095306	23612.845048	29.982260
405.518205	23649.035610	29.987277
405.656155	23699.621707	29.992295
406.218364	23735.570273	29.997312
406.433006	23773.216156	30.002330
407.230395	23807.527197	30.007348
407.571100	23859.409481	30.012365
408.003820	23892.398117	30.017383
408.438556	23922.494694	30.022400
409.004200	23966.361709	30.027418
409.694119	24010.712875	30.032436
409.958605	24043.496235	30.037453
410.338861	24084.535483	30.042471
410.926673	24120.559477	30.047488
410.838498	24151.075545	30.052506
412.032398	24187.751686	30.057524
412.144287	24215.812870	30.062541
412.507236	24245.198131	30.067559
412.839016	24278.172658	30.072576
413.191202	24318.272606	30.077594
413.568792	24347.218851	30.082612
413.989113	24384.313345	30.087629
414.477789	24425.259820	30.092647
415.097873	24468.518375	30.097664
415.321467	24505.568368	30.102682
415.585942	24532.628816	30.107700
415.699133	24580.780707	30.112717
416.124046	24612.844861	30.117735
416.759100	24655.650447	30.122752
416.672532	24700.193187	30.127770
417.217264	24742.700122	30.132788
418.075404	24788.471499	30.137805
418.302385	24830.148110	30.142823
418.940273	24858.602824	30.147840
419.120773	24900.528544	30.152858
419.966208	24926.082359	30.157876
420.271279	24971.893559	30.162893
421.068290	25000.487796	30.167911
421.635813	25028.148640	30.172928
421.728531	25073.440135	30.177946
421.953936	25095.291637	30.182964
422.125394	25132.859362	30.187981
422.428330	25164.328147	30.192999
423.147546	25188.838814	30.198016
423.564647	25220.940098	30.203034
424.096921	25254.862646	30.208052
424.406560	25281.935749	30.213069
424.816219	25321.320543	30.218087
425.171750	25364.068438	30.223104
425.382641	25388.415792	30.228122
425.786586	25425.113152	30.233140
425.856594	25472.684934	30.238157
426.352919	25515.367373	30.243175
426.913472	25548.822223	30.248192
426.933346	25595.142671	30.253210
427.883956	25639.169603	30.258228
428.119731	25686.088557	30.263245
428.748430	25736.837758	30.268263
429.133379	25776.112569	30.273280
429.047194	25826.942287	30.278298
429.894355	25868.821759	30.283316
430.261542	25918.867229	30.288333
430.762238	25970.455131	30.293351
431.220624	26015.650872	30.298368
431.568527	26054.471970	30.303386
432.140102	26106.745593	30.308404
432.915295	26145.307075	30.313421
432.977206	26186.449711	30.318439
433.753770	26229.174373	30.323456
433.931239	26274.123885	30.328474
434.489379	26320.707469	30.333492
435.077190	26359.107996	30.338509
435.362928	26402.283188	30.343527
436.178924	26433.562323	30.348544
436.622095	26481.691873	30.353562
437.316684	26520.750081	30.358580
437.702198	26547.848928	30.363597
437.990364	26596.947459	30.368615
438.684673	26622.210233	30.373632
439.139918	26662.607764	30.378650
439.029253	26702.401831	30.383668
439.885624	26734.564289	30.388685
439.657653	26782.146353	30.393703
440.634272	26824.132945	30.398720
440.714952	26863.063101	30.403738
441.081321	26904.314868	30.408756
441.613091	26950.923447	30.413773
442.028847	26995.848103	30.418791
442.562851	27032.041695	30.423808
442.648790	27078.834663	30.428826
443.361879	27125.394838	30.433844
443.919286	27178.096724	30.438861
444.260214	27214.899802	30.443879
445.043570	27250.614238	30.448896
445.049642	27296.591451	30.453914
445.495782	27334.986026	30.458932
445.969199	27375.700805	30.463949
446.353293	27425.448234	30.468967
447.143784	27462.360520	30.473984
447.043820	27513.752643	30.479002
447.900479	27555.618905	30.484020
448.521358	27590.837291	30.489037
449.005832	27642.953350	30.494055
449.334005	27668.401165	30.499072
450.031157	27699.982972	30.504090
450.666264	27748.352476	30.509108
451.393734	27784.531465	30.514125
451.406955	27813.283549	30.519143
451.882781	27837.902890	30.524160
452.093684	27878.277404	30.529178
452.206338	27913.542555	30.534196
452.942624	27952.202851	30.539213
452.820872	27990.875648	30.544231
453.599434	28020.968393	30.549248
453.880890	28070.365587	30.554266
454.685154	28114.926175	30.559284
454.761270	28151.513193	30.564301
454.927583	28204.610874	30.569319
455.483810	28252.928584	30.574336
456.070773	28297.049234	30.579354
456.217528	28353.721317	30.584372
456.576436	28387.306494	30.589389
457.230482	28449.872597	30.594407
457.460241	28496.705587	30.599424
458.162073	28541.877221	30.604442
458.391068	28601.700378	30.609460
458.868973	28640.632016	30.614477
459.423824	28704.007180	30.619495
459.996332	28750.705378	30.624512
460.354401	28812.917922	30.629530
460.880822	28875.244828	30.634548
461.513986	28906.000334	30.639565
462.146468	28969.130216	30.644583
462.416262	29022.632856	30.649600
462.982923	29069.093140	30.654618
463.542505	29111.731478	30.659636
463.956499	29157.018511	30.664653
464.240620	29217.279470	30.669671
465.222060	29263.062937	30.674688
465.580689	29299.501613	30.679706
466.092263	29361.485723	30.684724
466.897697	29401.970627	30.689741
467.001202	29458.470503	30.694759
467.673262	29492.690633	30.699776
468.234131	29539.481208	30.704794
468.500878	29585.784217	30.709812
468.836192	29630.375704	30.714829
469.723770	29669.866590	30.719847
470.467563	29708.949138	30.724864
470.775711	29746.097410	30.729882
471.198222	29792.741174	30.734900
471.631279	29827.086619	30.739917
471.988034	29881.258938	30.744935
472.682620	29917.198611	30.749952
472.961158	29964.197854	30.754970
473.226343	30016.398295	30.759988
473.962419	30044.331184	30.765005
474.064293	30094.199152	30.770023
474.849936	30142.503162	30.775040
475.421110	30181.394461	30.780058
475.504828	30237.502644	30.785076
475.898824	30284.196602	30.790093
476.254206	30331.348186	30.795111
476.402017	30384.215832	30.800128
477.137453	30438.248461	30.805146
477.312442	30494.553760	30.810164
478.021294	30549.373500	30.815181
478.321086	30612.318237	30.820199
478.928599	30670.208904	30.825216
478.965411	30718.874817	30.830234
479.602598	30771.309461	30.835252
480.108025	30834.684784	30.840269
480.922091	30891.302228	30.845287
481.257180	30947.951654	30.850304
482.070752	30996.531043	30.855322
482.514377	31030.422819	30.860340
483.420470	31080.835893	30.865357
483.657456	31117.740145	30.870375
484.223130	31157.338061	30.875392
484.696890	31205.068718	30.880410
485.034975	31246.957006	30.885428
485.245973	31289.497364	30.890445
485.830710	31347.876735	30.895463
486.352291	31387.447752	30.900480
486.843943	31438.463495	30.905498
487.481965	31485.842829	30.910516
488.095502	31530.184988	30.915533
487.935541	31592.975732	30.920551
488.563712	31641.054354	30.925568
488.995738	31684.710715	30.930586
489.293340	31754.206446	30.935604
489.995920	31800.380235	30.940621
490.633694	31855.991937	30.945639
491.459420	31917.415817	30.950656
491.710083	31960.645349	30.955674
492.335789	32026.715265	30.960692
492.720530	32067.506172	30.965709
492.891043	32120.069269	30.970727
493.569131	32186.424551	30.975744
494.086152	32230.383733	30.980762
494.543861	32288.727273	30.985780
494.975562	32340.418104	30.990797
495.429869	32393.045567	30.995815
495.929531	32451.480524	31.000832
496.388590	32505.227594	31.005850
496.868136	32568.878488	31.010868
497.312305	32620.561773	31.015885
497.957964	32688.101163	31.020903
498.669233	32747.877788	31.025920
499.027037	32810.634674	31.030938
499.372402	32879.925032	31.035956
499.817592	32929.431988	31.040973
500.356189	32987.114514	31.045991
500.727175	33059.332511	31.051008
501.149044	33118.912092	31.056026
501.845785	33173.533794	31.061044
502.310356	33244.866250	31.066061
502.336885	33308.966963	31.071079
502.633297	33373.272593	31.076096
503.595214	33446.599868	31.081114
504.305821	33503.580440	31.086132
504.983752	33574.888451	31.091149
505.765419	33634.091652	31.096167
505.897264	33677.931906	31.101184
506.482851	33745.860747	31.106202
506.908771	33806.842940	31.111220
507.587402	33863.353498	31.116237
508.327027	33918.140807	31.121255
508.552983	33990.370783	31.126272
509.620878	34033.214816	31.131290
509.869362	34089.708799	31.136308
510.058258	34164.675012	31.141325
510.987047	34215.809602	31.146343
511.576034	34265.340721	31.151360
511.993972	34313.486604	31.156378
512.113086	34391.182118	31.161396
512.825277	34448.701895	31.166413
513.087163	34505.371691	31.171431
513.931218	34556.641168	31.176448
514.813109	34612.009816	31.181466
514.724878	34674.853296	31.186484
515.480738	34733.884572	31.191501
516.113234	34780.219735	31.196519
516.859414	34841.130491	31.201536
516.968722	34887.145292	31.206554
517.230076	34934.716017	31.211572
517.735077	34985.332742	31.216589
518.537346	35042.208453	31.221607
518.726047	35087.257680	31.226624
519.015630	35149.645982	31.231642
519.680316	35216.008531	31.236660
519.999271	35273.564375	31.241677
520.796379	35333.799420	31.246695
521.171849	35396.584627	31.251712
521.714615	35461.661806	31.256730
522.121504	35524.672634	31.261748
523.069533	35585.154984	31.266765
523.183561	35643.859816	31.271783
523.449264	35700.854660	31.276800
524.438915	35765.786551	31.281818
524.880404	35827.732425	31.286836
525.503434	35893.905568	31.291853
525.904237	35965.354146	31.296871
526.424850	36018.432681	31.301888
527.057128	36081.001153	31.306906
527.264816	36162.404047	31.311924
528.092426	36208.474013	31.316941
528.889527	36272.940942	31.321959
528.906371	36339.256886	31.326976
530.203287	36401.303287	31.331994
530.547519	36466.025596	31.337012
530.831893	36520.826685	31.342029
531.596247	36580.064639	31.347047
531.854483	36654.954116	31.352064
532.761796	36710.990963	31.357082
532.923231	36791.621703	31.362100
533.483429	36847.627949	31.367117
533.940822	36914.630657	31.372135
534.484558	36976.386883	31.377152
535.336925	37045.792746	31.382170
535.559054	37112.213338	31.387188
535.930522	37175.040153	31.392205
536.652109	37244.405267	31.397223
537.627383	37307.413689	31.402240
538.168542	37370.696019	31.407258
538.404134	37433.363135	31.412276
538.795579	37506.245891	31.417293
539.645271	37578.620878	31.422311
539.786047	37630.097397	31.427328
540.717948	37693.581425	31.432346
540.772989	37773.697612	31.437364
540.848767	37839.191934	31.442381
541.665231	37918.734837	31.447399
542.358429	37986.043435	31.452416
543.220993	38052.541601	31.457434
543.733383	38126.969147	31.462452
544.194604	38191.899262	31.467469
544.883834	38262.517144	31.472487
545.416195	38343.169299	31.477504
546.554309	38391.024132	31.482522
547.198207	38461.230512	31.487540
547.607359	38522.199977	31.492557
548.074010	38585.959675	31.497575
548.321923	38652.220708	31.502592
548.879984	38704.830711	31.507610
549.525772	38778.108984	31.512628
549.958926	38851.836140	31.517645
550.859395	38904.803632	31.522663
550.879301	38980.569056	31.527680
551.575933	39031.058218	31.532698
552.172435	39100.956125	31.537716
552.696002	39166.494908	31.542733
552.972588	39215.722018	31.547751
553.772848	39289.358752	31.552768
554.622363	39341.168108	31.557786
555.300825	39397.453110	31.562804
555.004141	39459.659647	31.567821
555.981754	39515.460031	31.572839
556.148020	39583.057293	31.577856
556.282261	39647.342765	31.582874
556.628116	39728.738910	31.587892
557.053022	39806.836565	31.592909
558.110537	39881.904082	31.597927
558.481683	39968.505178	31.602944
559.329551	40031.329500	31.607962
559.850309	40110.602596	31.612980
560.535443	40187.693030	31.617997
560.835437	40253.954451	31.623015
561.419282	40330.765513	31.628032
562.258024	40406.641509	31.633050
562.941056	40484.055504	31.638068
562.840635	40565.506999	31.643085
563.836948	40630.007070	31.648103
564.451909	40720.169900	31.653120
564.949082	40796.324891	31.658138
565.250421	40870.482871	31.663156
565.800565	40945.742739	31.668173
566.516749	41030.230627	31.673191
566.862866	41101.828463	31.678208
567.581500	41203.570773	31.683226
568.272455	41282.776646	31.688244
568.423165	41357.649624	31.693261
569.494981	41444.448171	31.698279
570.217925	41531.680398	31.703296
571.313736	41597.502723	31.708314
571.646870	41675.348881	31.713332
572.260865	41745.424486	31.718349
572.763721	41811.408653	31.723367
573.133494	41901.109553	31.728384
573.843450	41966.605499	31.733402
574.441392	42048.216545	31.738420
574.801305	42125.662432	31.743437
575.372392	42189.404839	31.748455
576.016766	42279.239006	31.753472
576.799743	42349.964561	31.758490
577.302123	42434.614182	31.763508
577.665383	42510.359598	31.768525
578.523651	42577.749429	31.773543
578.967206	42666.251730	31.778560
579.501236	42736.880986	31.783578
580.196257	42825.209925	31.788596
580.750520	42913.676184	31.793613
581.452776	42980.651287	31.798631
581.873155	43058.997143	31.803648
582.728268	43125.442413	31.808666
582.930892	43203.452326	31.813684
583.618493	43291.686853	31.818701
584.344719	43368.929072	31.823719
584.727858	43454.427036	31.828736
585.343944	43523.495650	31.833754
586.130203	43604.362669	31.838772
586.323882	43683.613638	31.843789
587.541562	43747.062042	31.848807
587.836678	43835.363985	31.853824
588.358024	43900.137087	31.858842
588.733270	43989.929302	31.863860
589.109162	44071.065033	31.868877
590.127684	44144.738865	31.873895
590.832820	44236.539389	31.878912
591.383145	44312.949535	31.883930
591.760093	44372.491468	31.888948
592.146101	44440.231285	31.893965
593.284550	44511.297878	31.898983
593.818629	44586.733103	31.904000
594.215367	44660.306460	31.909018
594.837662	44730.748770	31.914036
594.732827	44814.713929	31.919053
595.534303	44887.801421	31.924071
596.493420	44972.652397	31.929088
597.000535	45048.952723	31.934106
597.708873	45120.269489	31.939124
598.071892	45214.063599	31.944141
598.578090	45282.639098	31.949159
598.743620	45364.238282	31.954176
599.590000	45461.022724	31.959194
600.542820	45536.888331	31.964212
600.919565	45633.261842	31.969229
601.691292	45712.905883	31.974247
602.177833	45785.357435	31.979264
602.796072	45869.517325	31.984282
603.611554	45953.935498	31.989300
604.157923	46031.291086	31.994317
605.189866	46117.268754	31.999335
605.668581	46198.554616	32.004352
606.366187	46286.034402	32.009370
606.985441	46358.598864	32.014388
607.595166	46444.486735	32.019405
607.925192	46519.170918	32.024423
608.713821	46615.190949	32.029440
608.653856	46697.101563	32.034458
609.656860	46789.522194	32.039476
609.624634	46880.137613	32.044493
610.562599	46977.167357	32.049511
611.325677	47067.270248	32.054528
611.741547	47160.904316	32.059546
612.516812	47245.994881	32.064564
612.966811	47351.781216	32.069581
613.770014	47438.083735	32.074599
614.536665	47529.839713	32.079616
614.903310	47619.006568	32.084634
615.668992	47714.641275	32.089652
616.070655	47809.493472	32.094669
616.883511	47890.958802	32.099687
617.528740	47985.534820	32.104704
617.813539	48089.568424	32.109722
618.929529	48191.109591	32.114740
619.186740	48277.569275	32.119757
620.198187	48372.348838	32.124775
620.814494	48462.912088	32.129792
621.387133	48554.499816	32.134810
622.119419	48640.604797	32.139828
622.304892	48735.892068	32.144845
622.820507	48826.978948	32.149863
623.175380	48931.135063	32.154880
624.020907	49030.382207	32.159898
625.028262	49130.291577	32.164916
625.389135	49221.203792	32.169933
626.102378	49320.344820	32.174951
627.007669	49403.974078	32.179968
627.419054	49498.552038	32.184986
628.458008	49592.714169	32.190004
628.964119	49693.912495	32.195021
629.467512	49782.425829	32.200039
630.590594	49870.470886	32.205056
631.011563	49951.984511	32.210074
632.006506	50039.397784	32.215092
632.618312	50121.970164	32.220109
633.339544	50191.772258	32.225127
633.579358	50270.537998	32.230144
634.123817	50352.557187	32.235162
634.960087	50426.386747	32.240180
635.332119	50510.996375	32.245197
636.015329	50590.726086	32.250215
637.165287	50666.295465	32.255232
637.746254	50757.207056	32.260250
638.309166	50816.413285	32.265268
638.678915	50903.213681	32.270285
639.026207	50989.146496	32.275303
639.890925	51067.455413	32.280320
640.566785	51165.876298	32.285338
640.861150	51253.252902	32.290356
641.317391	51339.955710	32.295373
642.163586	51431.622585	32.300391
643.269849	51510.875659	32.305408
643.572266	51611.672418	32.310426
644.059944	51699.101235	32.315444
644.295706	51781.796552	32.320461
645.476551	51894.862226	32.325479
646.420296	51985.874468	32.330496
646.591973	52074.427884	32.335514
647.276777	52169.589741	32.340532
647.925243	52262.986162	32.345549
648.380850	52354.046015	32.350567
648.937594	52461.077970	32.355584
649.831669	52562.546330	32.360602
650.116053	52662.195524	32.365620
651.142552	52767.780781	32.370637
651.335054	52862.891537	32.375655
652.228506	52955.562267	32.380672
652.797640	53058.571429	32.385690
653.323913	53156.408073	32.390708
654.030457	53272.788248	32.395725
654.871856	53380.315231	32.400743
656.021441	53484.039401	32.405760
656.205712	53586.830645	32.410778
657.297714	53668.795604	32.415796
657.566756	53777.145812	32.420813
658.270903	53891.426373	32.425831
659.285729	53975.079502	32.430848
659.715571	54084.421981	32.435866
660.427300	54176.503105	32.440884
661.577362	54267.722569	32.445901
662.181663	54359.929701	32.450919
663.019531	54448.061704	32.455936
663.385847	54549.930846	32.460954
664.039579	54650.344195	32.465972
665.105548	54751.504968	32.470989
665.491573	54847.534790	32.476007
666.250595	54927.879502	32.481024
666.994763	55035.058912	32.486042
667.579154	55125.447079	32.491060
667.926938	55222.432736	32.496077
668.232696	55324.657073	32.501095
668.681271	55416.705361	32.506112
669.233987	55539.246566	32.511130
669.893210	55651.074476	32.516148
670.629030	55754.601040	32.521165
671.536418	55869.238662	32.526183
672.519125	55961.024376	32.531200
673.083898	56070.924280	32.536218
673.862611	56163.761857	32.541236
674.282525	56269.162947	32.546253
674.958065	56383.361665	32.551271
675.960293	56474.104027	32.556288
676.668574	56580.975553	32.561306
677.540334	56671.677188	32.566324
677.996293	56750.499802	32.571341
678.424297	56856.951547	32.576359
679.206886	56940.276569	32.581376
679.866219	57042.558830	32.586394
680.614436	57150.273516	32.591412
681.311395	57230.783200	32.596429
681.846255	57325.214556	32.601447
683.171340	57409.759907	32.606464
683.683085	57519.209041	32.611482
683.817689	57610.055676	32.616500
684.826327	57693.416038	32.621517
685.021576	57803.020105	32.626535
685.932383	57895.799763	32.631552
686.527232	57998.798987	32.636570
687.488925	58101.276884	32.641588
688.455733	58213.466567	32.646605
688.944648	58303.095177	32.651623
689.858821	58393.690263	32.656640
690.737197	58500.904217	32.661658
691.230021	58583.020196	32.666676
691.831194	58685.598554	32.671693
692.319255	58782.622715	32.676711
693.310743	58887.570484	32.681728
693.693463	58994.331825	32.686746
694.205397	59081.135481	32.691764
694.951083	59196.318250	32.696781
695.449564	59302.392281	32.701799
696.340882	59414.866590	32.706816
696.303861	59527.981430	32.711834
697.272232	59639.332078	32.716852
698.183375	59764.860797	32.721869
698.789707	59879.843010	32.726887
699.574291	59998.897754	32.731904
699.688018	60116.281906	32.736922
700.361869	60223.772681	32.741940
701.332456	60357.106191	32.746957
701.819475	60480.902034	32.751975
702.598026	60596.953190	32.756992
703.343191	60728.044999	32.762010
704.394547	60840.880035	32.767028
705.287895	60944.597145	32.772045
705.728626	61074.490174	32.777063
706.627456	61181.923623	32.782080
707.462124	61310.514428	32.787098
707.845408	61423.368251	32.792116
708.683172	61540.552626	32.797133
709.445178	61666.193650	32.802151
710.395842	61776.958633	32.807168
710.927445	61897.469389	32.812186
711.745939	62018.894130	32.817204
712.705994	62120.097180	32.822221
713.099696	62241.530204	32.827239
714.309966	62355.674665	32.832256
714.451860	62482.295331	32.837274
714.684491	62597.152459	32.842292
715.769209	62714.972772	32.847309
716.755862	62848.143057	32.852327
717.577397	62956.041082	32.857344
717.899754	63087.584540	32.862362
718.330473	63206.767138	32.867380
719.629848	63317.293303	32.872397
720.132998	63447.336548	32.877415
720.790810	63556.370870	32.882432
721.524072	63678.255685	32.887450
722.360409	63804.927873	32.892468
723.311812	63914.699373	32.897485
723.984275	64037.753046	32.902503
724.766602	64139.134513	32.907520
725.286416	64245.559550	32.912538
726.014150	64353.752224	32.917556
726.830587	64455.679528	32.922573
727.621159	64578.546273	32.927591
728.432499	64680.842145	32.932608
729.056176	64794.566136	32.937626
729.499590	64906.740286	32.942644
730.183401	65016.327985	32.947661
730.564858	65149.347678	32.952679
731.471006	65258.735599	32.957696
732.213189	65388.328132	32.962714
733.157231	65505.985431	32.967732
734.117830	65610.416771	32.972749
734.297048	65749.561012	32.977767
734.994801	65854.877715	32.982784
736.145569	65988.970472	32.987802
736.501491	66118.100373	32.992820
737.565776	66224.034802	32.997837
738.089764	66361.526906	33.002855
738.928033	66483.815526	33.007872
739.544154	66615.946161	33.012890
740.038462	66751.808482	33.017908
740.935504	66871.719107	33.022925
741.458568	67011.112120	33.027943
742.007893	67129.298960	33.032960
742.716308	67277.943304	33.037978
743.457844	67423.662601	33.042996
744.742037	67547.590687	33.048013
745.073149	67685.995778	33.053031
746.111558	67820.978655	33.058048
746.807683	67951.113148	33.063066
747.407691	68088.648326	33.068084
748.730941	68222.651107	33.073101
749.518319	68355.504129	33.078119
750.456442	68480.696070	33.083136
751.343992	68611.561691	33.088154
752.007008	68734.714291	33.093172
753.037898	68866.265904	33.098189
753.217537	68995.531193	33.103207
754.048786	69130.190010	33.108224
754.840478	69249.183305	33.113242
755.593043	69391.905039	33.118260
756.175769	69519.159696	33.123277
756.797736	69658.086095	33.128295
757.321575	69788.228785	33.133312
758.702367	69919.280287	33.138330
759.495193	70061.424546	33.143348
760.082155	70182.126044	33.148365
760.841955	70319.213125	33.153383
761.668376	70449.240356	33.158400
762.828050	70586.655132	33.163418
763.262237	70719.385345	33.168436
764.290306	70841.073636	33.173453
764.381122	70988.322353	33.178471
764.822634	71123.418597	33.183488
765.644270	71262.012699	33.188506
766.891879	71412.184162	33.193524
767.744951	71545.779814	33.198541
768.441367	71683.967374	33.203559
768.908702	71829.300750	33.208576
769.672646	71954.573590	33.213594
770.576161	72101.000227	33.218612
771.355507	72237.717026	33.223629
772.013150	72375.561355	33.228647
773.014449	72505.382538	33.233664
773.604508	72654.160050	33.238682
774.684993	72791.064606	33.243700
775.604255	72921.850352	33.248717
776.082556	73054.132477	33.253735
776.784119	73185.063270	33.258752
777.681237	73303.119590	33.263770
778.168439	73438.267135	33.268788
779.349970	73565.194075	33.273805
780.085350	73695.540616	33.278823
780.897515	73824.104647	33.283840
781.651564	73952.691688	33.288858
781.788727	74079.256600	33.293876
782.695169	74225.848968	33.298893
783.690546	74369.240454	33.303911
784.356998	74499.754989	33.308928
785.093844	74646.024069	33.313946
785.386560	74804.635856	33.318964
786.686317	74931.968662	33.323981
787.072513	75084.818588	33.328999
787.841936	75238.308269	33.334016
788.864146	75374.745518	33.339034
789.752294	75527.174155	33.344052
790.864806	75670.371474	33.349069
791.823865	75808.630575	33.354087
792.640434	75953.054920	33.359104
793.599368	76090.398808	33.364122
794.105697	76231.903811	33.369140
794.972647	76359.139337	33.374157
795.984626	76505.223657	33.379175
796.678395	76639.300787	33.384192
798.055947	76774.853263	33.389210
798.750002	76932.067088	33.394228
799.304811	77061.356777	33.399245
800.007024	77203.335330	33.404263
801.068442	77346.672200	33.409280
801.830503	77478.263904	33.414298
802.400700	77626.079360	33.419316
803.144446	77770.369552	33.424333
804.008063	77922.926387	33.429351
804.737651	78061.439942	33.434368
805.522513	78220.368305	33.439386
805.908365	78367.257769	33.444404
807.001432	78516.226188	33.449421
807.714508	78662.797923	33.454439
808.184627	78808.771915	33.459456
809.294634	78962.066868	33.464474
809.479460	79119.348694	33.469492
811.139671	79266.685153	33.474509
811.953687	79419.633647	33.479527
812.847204	79562.063780	33.484544
813.839771	79707.944738	33.489562
814.595014	79862.310190	33.494580
815.379006	80009.498955	33.499597
816.304733	80154.919461	33.504615
817.008905	80292.938731	33.509632
817.888893	80440.209357	33.514650
818.804291	80592.168670	33.519668
819.767777	80738.744305	33.524685
820.572486	80880.229668	33.529703
820.867839	81029.371878	33.534720
821.870146	81164.424803	33.539738
822.216654	81318.595756	33.544756
823.195434	81476.490472	33.549773
823.893784	81624.665479	33.554791
824.689183	81783.977988	33.559808
826.303524	81935.362828	33.564826
826.818922	82091.680964	33.569844
827.685184	82243.014265	33.574861
828.810935	82382.457003	33.579879
829.249450	82537.645890	33.584896
830.537037	82660.919392	33.589914
831.279158	82799.403206	33.594932
831.925161	82928.389101	33.599949
833.224881	83065.207229	33.604967
833.600604	83206.575532	33.609984
834.633512	83337.707734	33.615002
835.213049	83484.402507	33.620020
835.684275	83616.185778	33.625037
836.640461	83767.261311	33.630055
837.235023	83932.233597	33.635072
838.162779	84072.389984	33.640090
838.603325	84220.542224	33.645108
839.320015	84377.589331	33.650125
840.193411	84537.623128	33.655143
840.814125	84707.873110	33.660160
841.524325	84876.053380	33.665178
842.507793	85046.758435	33.670196
842.941731	85206.388612	33.675213
843.978849	85375.480225	33.680231
844.826235	85537.942140	33.685248
845.736538	85705.899283	33.690266
846.694406	85880.815851	33.695284
847.620096	86048.798250	33.700301
848.713794	86217.405818	33.705319
849.664733	86396.680485	33.710336
850.621805	86551.526140	33.715354
851.475716	86726.200506	33.720372
852.627688	86874.840726	33.725389
853.475057	87045.741172	33.730407
853.922495	87211.020584	33.735424
854.963374	87368.123038	33.740442
856.039427	87536.781044	33.745460
856.436967	87713.480699	33.750477
857.426123	87874.442234	33.755495
858.641334	88045.314561	33.760512
859.257897	88207.877522	33.765530
860.159109	88365.946229	33.770548
861.142591	88541.074682	33.775565
862.428123	88700.664119	33.780583
862.878031	88871.466338	33.785600
864.062289	89022.380228	33.790618
864.514811	89195.240921	33.795636
865.195296	89372.083499	33.800653
866.563249	89532.924227	33.805671
867.164929	89707.352367	33.810688
867.815403	89876.464450	33.815706
868.927914	90046.697467	33.820724
869.357071	90220.923730	33.825741
870.775676	90402.303344	33.830759
871.353998	90576.324061	33.835776
872.088789	90750.288572	33.840794
873.083915	90918.401907	33.845812
873.873401	91099.764148	33.850829
874.755417	91278.163416	33.855847
875.476339	91452.489729	33.860864
876.342678	91629.407001	33.865882
877.524437	91807.279748	33.870900
878.532427	91982.492824	33.875917
879.344827	92161.568347	33.880935
879.907206	92338.319531	33.885952
881.042427	92516.369763	33.890970
881.860771	92693.435702	33.895988
882.421278	92873.602375	33.901005
884.232768	93040.817332	33.906023
884.992265	93220.820830	33.911040
885.884918	93385.132986	33.916058
886.823354	93566.179114	33.921076
887.789891	93723.576339	33.926093
889.160453	93873.009078	33.931111
889.660863	94030.124496	33.936128
890.578322	94177.418704	33.941146
891.639396	94331.582677	33.946164
892.367950	94486.302547	33.951181
893.261732	94648.895163	33.956199
893.881469	94801.919746	33.961216
894.987613	94965.833901	33.966234
895.588352	95121.281469	33.971252
896.522139	95274.276143	33.976269
897.724393	95437.380068	33.981287
898.315285	95603.035584	33.986304
899.254756	95760.513719	33.991322
900.262923	95933.444961	33.996340
900.885901	96097.161625	34.001357
901.795339	96266.978293	34.006375
902.148409	96444.262245	34.011392
902.925020	96615.964218	34.016410
903.930715	96802.542841	34.021428
904.488243	96984.879836	34.026445
905.694826	97157.881849	34.031463
906.627011	97353.971782	34.036480
907.577257	97532.968995	34.041498
908.866338	97712.816762	34.046516
909.432573	97904.521371	34.051533
910.846738	98082.559713	34.056551
911.549078	98254.943638	34.061568
912.460400	98439.891611	34.066586
913.519829	98618.600064	34.071604
914.219903	98804.300947	34.076621
915.276754	98985.411678	34.081639
916.335421	99175.487435	34.086656
916.988351	99353.426291	34.091674
918.144167	99547.622684	34.096692
918.491691	99733.141756	34.101709
919.757125	99920.663074	34.106727
920.616156	100116.128351	34.111744
921.506944	100300.447681	34.116762
922.857376	100493.365728	34.121780
923.541904	100682.729605	34.126797
924.343491	100868.087074	34.131815
925.143225	101067.646620	34.136832
926.153312	101250.218470	34.141850
927.408336	101446.318710	34.146868
928.123687	101633.519354	34.151885
929.100343	101822.355991	34.156903
930.002587	102023.799129	34.161920
930.632769	102203.591482	34.166938
932.150550	102392.855823	34.171956
933.048084	102589.758307	34.176973
934.022194	102765.825624	34.181991
935.495579	102960.584496	34.187008
936.072516	103147.559476	34.192026
937.402243	103333.645401	34.197044
937.854008	103524.733970	34.202061
938.650904	103709.549291	34.207079
939.875607	103908.294674	34.212096
940.249517	104100.843984	34.217114
941.239174	104287.030919	34.222132
942.259852	104493.184681	34.227149
943.555512	104684.465398	34.232167
944.131203	104883.566028	34.237184
945.175340	105057.978432	34.242202
946.102734	105256.599601	34.247220
946.585744	105462.704180	34.252237
947.769320	105655.143972	34.257255
948.796748	105847.053730	34.262272
949.530903	106044.028431	34.267290
950.539264	106240.389433	34.272308
950.888954	106425.741123	34.277325
952.116703	106617.306824	34.282343
952.710209	106817.945318	34.287360
953.498203	107022.074068	34.292378
954.713560	107217.774938	34.297396
955.614992	107415.251541	34.302413
956.993622	107609.319886	34.307431
957.712002	107810.616551	34.312448
958.346483	108017.298713	34.317466
959.662549	108209.481973	34.322484
960.424222	108419.147973	34.327501
961.403597	108629.311637	34.332519
962.139487	108836.274722	34.337536
962.909023	109053.860514	34.342554
964.100905	109260.067635	34.347572
965.125468	109469.736472	34.352589
966.290762	109686.983410	34.357607
967.187440	109896.752693	34.362624
967.839104	110101.611517	34.367642
968.501035	110327.331866	34.372660
969.794027	110561.436515	34.377677
970.724597	110774.829673	34.382695
971.759911	110992.425256	34.387712
972.822831	111227.156322	34.392730
973.770791	111429.632908	34.397748
974.671027	111668.093402	34.402765
975.567821	111875.205241	34.407783
976.894782	112103.820025	34.412800
977.677698	112336.314101	34.417818
978.849057	112552.632951	34.422836
979.811555	112782.073630	34.427853
981.123033	113005.973489	34.432871
982.022423	113233.920904	34.437888
982.871208	113460.827125	34.442906
983.883062	113678.333952	34.447924
985.085455	113910.037338	34.452941
985.956730	114138.110878	34.457959
987.678981	114344.281606	34.462976
988.385514	114573.006673	34.467994
989.664290	114787.779770	34.473012
990.242951	115006.280676	34.478029
991.448992	115235.828193	34.483047
992.344438	115445.551483	34.488064
992.899338	115675.526839	34.493082
994.103806	115901.558121	34.498100
995.373184	116125.996868	34.503117
996.621732	116340.140762	34.508135
997.433796	116566.191504	34.513152
998.623651	116770.783022	34.518170
1000.013660	116990.837801	34.523188
1001.037860	117216.301270	34.528205
1002.119883	117418.584073	34.533223
1003.226054	117638.361339	34.538240
1003.836143	117844.234632	34.543258
1005.337142	118046.135989	34.548276
1006.436776	118266.869444	34.553293
1007.533936	118464.329888	34.558311
1008.740055	118678.663180	34.563328
1009.357866	118886.595310	34.568346
1010.633796	119087.996372	34.573364
1011.132624	119305.339992	34.578381
1011.753301	119511.274229	34.583399
1013.122227	119725.841883	34.588416
1013.755225	119947.539606	34.593434
1014.629849	120160.152096	34.598452
1015.503928	120390.125542	34.603469
1016.466826	120602.346578	34.608487
1017.487000	120818.132994	34.613504
1018.188143	121036.660002	34.618522
1019.312382	121244.981677	34.623540
1020.460214	121469.076958	34.628557
1020.929433	121690.586948	34.633575
1022.200421	121890.893235	34.638592
1023.051488	122119.705680	34.643610
1024.313313	122337.212142	34.648628
1025.732638	122539.627250	34.653645
1027.454488	122755.223426	34.658663
1028.315793	122974.992999	34.663680
1028.922551	123193.716421	34.668698
1029.983795	123406.549826	34.673716
1030.769235	123616.363570	34.678733
1031.672872	123855.230041	34.683751
1032.907122	124061.677982	34.688768
1033.428322	124294.046707	34.693786
1034.582552	124524.994761	34.698804
1035.522423	124762.278428	34.703821
1036.476980	124994.492351	34.708839
1037.999520	125226.779054	34.713856
1038.695652	125465.502575	34.718874
1039.642323	125698.547009	34.723892
1040.799375	125939.099190	34.728909
1041.345288	126182.301560	34.733927
1042.745456	126426.277355	34.738944
1043.264329	126682.377275	34.743962
1044.533566	126910.916658	34.748980
1045.712817	127162.272987	34.753997
1046.522140	127403.768707	34.759015
1047.958672	127648.977702	34.764032
1049.171035	127903.249722	34.769050
1050.180771	128133.615506	34.774068
1051.508467	128391.396000	34.779085
1052.312229	128638.884713	34.784103
1053.733527	128874.283269	34.789120
1054.873396	129131.340492	34.794138
1056.280325	129357.010912	34.799156
1057.147196	129604.902548	34.804173
1058.091083	129844.608060	34.809191
1059.287418	130084.058268	34.814208
1060.355498	130325.166595	34.819226
1061.388088	130560.756209	34.824244
1062.160412	130810.067336	34.829261
1063.502528	131065.434007	34.834279
1064.876651	131296.561697	34.839296
1065.823836	131555.990377	34.844314
1066.908040	131784.304804	34.849332
1068.221107	132019.149217	34.854349
1069.421921	132267.513847	34.859367
1070.615506	132493.140704	34.864384
1071.677975	132738.312138	34.869402
1073.381067	132960.930008	34.874420
1074.314745	133176.869250	34.879437
1075.639480	133403.849968	34.884455
1076.722317	133623.355045	34.889472
1077.708703	133861.398109	34.894490
1079.166042	134082.543177	34.899508
1079.630737	134303.714198	34.904525
1080.543751	134535.055660	34.909543
1081.669838	134767.263673	34.914560
1082.327277	135001.807245	34.919578
1083.056533	135240.955153	34.924596
1084.347322	135471.898670	34.929613
1085.117783	135724.962985	34.934631
1086.189474	135947.743799	34.939648
1087.260214	136194.372753	34.944666
1088.671978	136431.667237	34.949684
1089.830710	136659.141941	34.954701
1090.409974	136883.049997	34.959719
1092.127329	137115.937819	34.964736
1092.869261	137348.886896	34.969754
1093.831455	137580.660228	34.974772
1094.700543	137817.699320	34.979789
1095.906715	138055.166236	34.984807
1097.436172	138277.697098	34.989824
1098.257784	138518.717362	34.994842
1099.149242	138754.656428	34.999860
1100.230048	138990.603939	35.004877
1100.809215	139245.958289	35.009895
1102.154139	139476.122165	35.014912
1102.612361	139742.315281	35.019930
1103.805184	139988.876250	35.024948
1104.935587	140256.255720	35.029965
1106.099212	140515.136761	35.034983
1107.272470	140757.509758	35.040000
1108.505016	141036.099696	35.045018
1109.579923	141289.447721	35.050036
1110.876759	141544.193786	35.055053
1111.760061	141808.114025	35.060071
1113.009640	142078.620035	35.065088
1114.116992	142334.481045	35.070106
1114.951404	142605.960016	35.075124
1116.460130	142864.789223	35.080141
1117.535688	143150.320226	35.085159
1118.590387	143411.193902	35.090176
1120.302804	143677.768569	35.095194
1121.031507	143952.521724	35.100212
1122.255073	144200.591542	35.105229
1123.362024	144473.473039	35.110247
1125.007712	144731.088873	35.115264
1126.151343	145002.218490	35.120282
1127.110443	145264.009445	35.125300
1128.560660	145524.415124	35.130317
1129.691816	145795.464133	35.135335
1130.709890	146055.691440	35.140352
1131.570402	146317.734729	35.145370
1132.491063	146581.063521	35.150388
1133.996243	146854.544421	35.155405
1134.735450	147128.115814	35.160423
1135.812647	147396.294505	35.165440
1136.842734	147677.494495	35.170458
1138.178875	147960.675260	35.175476
1139.368218	148223.895663	35.180493
1140.345081	148510.627593	35.185511
1141.972319	148778.193103	35.190528
1143.225510	149045.733554	35.195546
1144.609252	149323.527137	35.200564
1145.997705	149574.130855	35.205581
1146.897778	149838.615519	35.210599
1148.029719	150112.804081	35.215616
1149.258465	150387.435283	35.220634
1150.357497	150653.300740	35.225652
1151.310479	150920.853680	35.230669
1152.449249	151187.642266	35.235687
1153.795372	151462.591823	35.240704
1155.275588	151716.670102	35.245722
1156.087272	151992.878643	35.250740
1157.338559	152260.125606	35.255757
1158.388396	152526.672085	35.260775
1159.562822	152786.984944	35.265792
1160.920882	153065.394212	35.270810
1161.507352	153327.951390	35.275828
1162.912437	153598.581687	35.280845
1163.696058	153888.152116	35.285863
1164.809038	154141.736572	35.290880
1166.217508	154414.997697	35.295898
1167.519623	154680.299977	35.300916
1168.491869	154934.191963	35.305933
1169.668409	155206.050997	35.310951
1170.768571	155456.081945	35.315968
1172.169750	155699.925512	35.320986
1173.490668	155970.954280	35.326004
1175.018467	156220.069695	35.331021
1175.814293	156482.588486	35.336039
1176.903861	156741.115561	35.341056
1178.205155	157014.400035	35.346074
1178.902081	157285.769254	35.351092
1180.501190	157547.959614	35.356109
1181.016214	157820.529570	35.361127
1182.249456	158098.678539	35.366144
1183.699127	158377.808563	35.371162
1184.210220	158657.881975	35.376180
1185.235296	158946.042009	35.381197
1186.419265	159244.212241	35.386215
1187.627651	159521.626775	35.391232
1188.670681	159827.841991	35.396250
1189.773709	160112.077589	35.401268
1191.261951	160416.980554	35.406285
1192.129532	160720.808451	35.411303
1193.448091	161012.169742	35.416320
1194.400770	161320.174503	35.421338
1195.749065	161632.619945	35.426356
1197.021992	161931.086999	35.431373
1198.137951	162232.461977	35.436391
1199.263921	162551.294371	35.441408
1200.753847	162860.871221	35.446426
1201.652066	163163.278468	35.451444
1203.357611	163474.004157	35.456461
1204.345237	163790.458336	35.461479
1205.552049	164100.382893	35.466496
1206.985877	164408.229608	35.471514
1208.405237	164720.026714	35.476532
1209.823692	165017.793962	35.481549
1210.918050	165332.541940	35.486567
1212.309282	165635.608692	35.491584
1213.754048	165930.523248	35.496602
1214.883568	166238.154274	35.501620
1216.468638	166546.981087	35.506637
1217.621676	166857.974932	35.511655
1219.099249	167147.208169	35.516672
1220.257116	167444.895647	35.521690
1221.324925	167757.825894	35.526708
1222.692249	168050.280741	35.531725
1223.780853	168350.130123	35.536743
1224.784862	168661.922687	35.541760
1226.222503	168946.301986	35.546778
1227.324227	169251.865167	35.551796
1228.498979	169567.137970	35.556813
1229.641319	169887.189348	35.561831
1230.503437	170193.750176	35.566848
1231.716255	170501.041922	35.571866
1233.123812	170816.170855	35.576884
1234.636268	171120.854151	35.581901
1235.969647	171427.586641	35.586919
1237.078661	171743.558010	35.591936
1238.474857	172048.748885	35.596954
1239.411948	172358.864966	35.601972
1241.005328	172658.824630	35.606989
1242.519658	172963.811715	35.612007
1243.618436	173259.060197	35.617024
1245.102578	173567.127145	35.622042
1246.283198	173878.850165	35.627060
1247.829933	174167.406290	35.632077
1249.303030	174465.037070	35.637095
1250.047786	174748.589633	35.642112
1251.617594	175025.954460	35.647130
1252.825950	175320.207937	35.652148
1253.858711	175583.997174	35.657165
1254.956869	175872.371202	35.662183
1255.888473	176172.462451	35.667200
1257.303155	176451.663197	35.672218
1258.764876	176746.797313	35.677236
1260.190724	177032.586039	35.682253
1261.192864	177315.857443	35.687271
1262.411507	177602.610140	35.692288
1263.875123	177897.002134	35.697306
1264.884666	178201.001837	35.702324
1266.145591	178506.789444	35.707341
1267.225848	178804.841719	35.712359
1268.033790	179110.987018	35.717376
1269.230668	179429.444101	35.722394
1270.209559	179744.271350	35.727412
1271.484423	180065.740162	35.732429
1273.045656	180378.964956	35.737447
1274.160486	180703.675213	35.742464
1275.514757	181035.315812	35.747482
1276.543095	181365.019731	35.752500
1277.848254	181685.643400	35.757517
1278.915032	182022.389218	35.762535
1280.090036	182354.892882	35.767552
1281.231133	182697.761103	35.772570
1282.495309	183040.649335	35.777588
1283.347132	183389.877895	35.782605
1284.805589	183729.641608	35.787623
1285.805042	184093.180224	35.792640
1286.596736	184455.994055	35.797658
1288.107253	184814.300023	35.802676
1289.405581	185185.755060	35.807693
1290.522398	185550.870782	35.812711
1291.643084	185927.983176	35.817728
1293.264602	186298.948231	35.822746
1294.853831	186671.165054	35.827764
1295.971130	187044.223878	35.832781
1297.617848	187406.865477	35.837799
1298.927085	187778.653611	35.842816
1300.203656	188145.702245	35.847834
1301.574569	188512.293430	35.852852
1303.309436	188882.901581	35.857869
1304.903179	189240.943269	35.862887
1305.841947	189606.571956	35.867904
1307.287255	189970.329529	35.872922
1308.825407	190339.646723	35.877940
1310.004808	190700.063485	35.882957
1312.098417	191060.128480	35.887975
1313.062897	191422.933585	35.892992
1314.631526	191780.779302	35.898010
1316.079602	192134.940328	35.903028
1317.497813	192495.189023	35.908045
1318.801865	192838.118036	35.913063
1320.238864	193197.796597	35.918080
1321.877936	193552.493032	35.923098
1323.442369	193897.276583	35.928116
1324.800938	194251.502900	35.933133
1325.668478	194594.450397	35.938151
1327.015028	194950.244186	35.943168
1328.227908	195300.260456	35.948186
1329.510817	195656.614673	35.953204
1330.560354	195999.920726	35.958221
1332.469502	196351.135544	35.963239
1333.211001	196721.016678	35.968256
1335.064419	197050.929158	35.973274
1336.413147	197379.047710	35.978292
1337.917567	197714.924574	35.983309
1339.334627	198032.650255	35.988327
1340.325141	198368.348708	35.993344
1341.761180	198697.475159	35.998362
1342.788478	199023.979218	36.003380
1343.874085	199363.488470	36.008397
1344.987430	199701.788768	36.013415
1346.273139	200048.200426	36.018432
1347.256993	200407.981799	36.023450
1348.555628	200754.902791	36.028468
1349.749703	201120.049072	36.033485
1351.285489	201485.090117	36.038503
1352.038894	201848.370477	36.043520
1353.258137	202227.535159	36.048538
1354.600390	202604.942189	36.053556
1355.324970	202978.161778	36.058573
1356.528589	203364.927670	36.063591
1358.084209	203763.559693	36.068608
1359.511418	204160.069385	36.073626
1360.716650	204551.285251	36.078644
1361.910037	204959.722076	36.083661
1363.668756	205357.199328	36.088679
1365.131330	205756.505174	36.093696
1366.504583	206152.425102	36.098714
1367.873677	206570.428073	36.103732
1369.437893	206969.266516	36.108749
1370.912163	207366.268101	36.113767
1372.041406	207766.439527	36.118784
1374.158079	208161.015590	36.123802
1375.811525	208566.056609	36.128820
1377.201497	208951.208134	36.133837
1378.684369	209346.123327	36.138855
1380.036143	209738.294036	36.143872
1381.463382	210137.133191	36.148890
1382.893670	210527.275857	36.153908
1384.034253	210923.817108	36.158925
1385.314278	211326.673499	36.163943
1386.871407	211727.556034	36.168960
1388.432445	212123.347956	36.173978
1390.251883	212529.359123	36.178996
1391.528522	212924.008119	36.184013
1393.100098	213315.537304	36.189031
1394.528951	213703.180770	36.194048
1396.105652	214098.699896	36.199066
1397.638011	214485.872617	36.204084
1398.770565	214889.595535	36.209101
1400.473217	215274.915025	36.214119
1400.954000	215669.631536	36.219136
1402.841857	216078.720895	36.224154
1404.274443	216482.909359	36.229172
1405.395552	216892.281260	36.234189
1406.475475	217287.261395	36.239207
1407.626449	217707.959198	36.244224
1409.396430	218110.879921	36.249242
1410.472603	218526.234764	36.254260
1411.958826	218945.765165	36.259277
1413.585384	219369.058508	36.264295
1414.703176	219837.316104	36.269312
1416.177218	220246.821776	36.274330
1417.678575	220670.547668	36.279348
1418.708045	221087.038444	36.284365
1420.181502	221496.574626	36.289383
1421.411897	221933.837048	36.294400
1422.598259	222354.218384	36.299418
1424.101371	222781.152805	36.304436
1425.562921	223207.156016	36.309453
1427.047045	223634.274725	36.314471
1428.332417	224051.750815	36.319488
1429.536446	224477.039458	36.324506
1431.105350	224882.000825	36.329524
1432.446359	225298.964364	36.334541
1434.043246	225716.903163	36.339559
1435.206420	226142.255517	36.344576
1436.326089	226558.625090	36.349594
1437.890490	226986.581216	36.354612
1439.670688	227419.227618	36.359629
1440.798602	227832.196621	36.364647
1442.472398	228277.868367	36.369664
1443.777512	228707.244844	36.374682
1445.332471	229139.908962	36.379700
1446.728559	229564.599650	36.384717
1447.801772	229993.510656	36.389735
1449.758469	230437.847732	36.394752
1451.007288	230887.789608	36.399770
1452.544121	231325.340723	36.404788
1454.042238	231768.843370	36.409805
1455.420002	232220.495523	36.414823
1457.096275	232662.117295	36.419840
1458.718294	233114.468558	36.424858
1460.456648	233561.899605	36.429876
1461.438715	234002.192075	36.434893
1463.217001	234448.857114	36.439911
1464.807481	234891.439426	36.444928
1466.433801	235342.348691	36.449946
1467.992029	235779.604510	36.454964
1469.219745	236235.789315	36.459981
1470.993863	236674.205739	36.464999
1472.442138	237128.857874	36.470016
1473.936428	237576.035521	36.475034
1475.878349	238018.034687	36.480052
1476.791625	238461.500176	36.485069
1478.761873	238901.642484	36.490087
1480.147239	239362.686496	36.495104
1481.656340	239809.689318	36.500122
1483.229179	240264.938297	36.505140
1484.125374	240714.355888	36.510157
1485.934515	241172.235132	36.515175
1487.178834	241617.075657	36.520192
1488.716073	242081.123660	36.525210
1490.237499	242530.772157	36.530228
1491.583100	243010.171301	36.535245
1493.035727	243474.642575	36.540263
1494.206044	243948.966686	36.545280
1495.785561	244420.048881	36.550298
1497.147821	244886.392135	36.555316
1498.381409	245365.331740	36.560333
1500.339978	245822.230105	36.565351
1501.719585	246312.781690	36.570368
1503.009929	246790.444276	36.575386
1504.862817	247264.814061	36.580404
1506.016099	247747.479730	36.585421
1507.714230	248227.338125	36.590439
1509.218080	248706.619613	36.595456
1510.471302	249184.368153	36.600474
1512.232367	249676.030548	36.605492
1513.305832	250165.266762	36.610509
1514.856544	250658.743349	36.615527
1516.676741	251146.765220	36.620544
1518.098845	251640.924668	36.625562
1519.698155	252107.340654	36.630580
1521.040558	252617.010172	36.635597
1522.649390	253111.877020	36.640615
1524.284920	253592.564956	36.645632
1525.242606	254086.727217	36.650650
1527.229500	254573.683354	36.655668
1528.514150	255069.519832	36.660685
1529.911664	255537.673911	36.665703
1531.587817	256014.952857	36.670720
1532.955608	256500.564408	36.675738
1534.541903	256981.872395	36.680756
1535.940384	257450.840189	36.685773
1537.385011	257927.954996	36.690791
1539.124762	258414.115638	36.695808
1540.608957	258910.860949	36.700826
1542.038635	259393.008463	36.705844
1543.103461	259896.859873	36.710861
1544.898475	260387.990802	36.715879
1546.420589	260892.325694	36.720896
1547.609345	261406.851500	36.725914
1549.283227	261898.662865	36.730932
1550.774873	262418.752697	36.735949
1552.998001	262924.140224	36.740967
1554.653747	263437.801092	36.745984
1555.617339	263952.439704	36.751002
1557.425495	264451.087108	36.756020
1558.908030	264974.479974	36.761037
1560.490269	265480.023028	36.766055
1562.155129	266003.664645	36.771072
1563.694390	266534.922188	36.776090
1565.416003	267047.960559	36.781108
1566.945452	267567.660454	36.786125
1568.402407	268083.358160	36.791143
1570.475497	268606.523846	36.796160
1572.469666	269117.762574	36.801178
1573.935714	269638.461634	36.806196
1575.634433	270154.726984	36.811213
1577.275168	270658.401397	36.816231
1578.605015	271185.954471	36.821248
1580.434195	271719.597350	36.826266
1581.915554	272232.872925	36.831284
1583.355683	272778.263768	36.836301
1584.972155	273296.418221	36.841319
1586.652934	273813.926166	36.846336
1587.940584	274354.512989	36.851354
1589.550210	274873.250207	36.856372
1590.800921	275407.439709	36.861389
1592.322964	275950.474318	36.866407
1594.103994	276491.255072	36.871424
1595.605461	277037.161318	36.876442
1597.462610	277574.624885	36.881460
1599.237118	278118.807118	36.886477
1600.528069	278651.713045	36.891495
1602.216228	279205.610643	36.896512
1603.902391	279747.415743	36.901530
1605.307529	280290.688362	36.906548
1607.039964	280839.875042	36.911565
1608.725467	281385.206877	36.916583
1610.353037	281929.606894	36.921600
1612.191687	282477.958630	36.926618
1613.858226	283019.046856	36.931636
1615.558455	283562.642689	36.936653
1616.795885	284101.994956	36.941671
1618.924348	284647.752132	36.946688
1620.249577	285201.463735	36.951706
1622.013975	285740.723870	36.956724
1623.881228	286284.969301	36.961741
1625.423863	286821.138059	36.966759
1627.250179	287367.164598	36.971776
1628.661826	287928.371207	36.976794
1630.039817	288472.918273	36.981812
1631.385273	289021.304214	36.986829
1632.947939	289574.249760	36.991847
1634.685688	290118.655051	36.996864
1636.084482	290664.028550	37.001882
1637.954918	291189.128720	37.006900
1639.273746	291723.309554	37.011917
1640.930821	292245.113310	37.016935
1643.456749	292767.355810	37.021952
1644.826190	293299.667581	37.026970
1646.690590	293824.808855	37.031988
1648.281945	294350.831135	37.037005
1649.754981	294898.841374	37.042023
1651.446906	295416.587511	37.047040
1653.164101	295962.622180	37.052058
1654.872588	296498.826173	37.057076
1656.655456	297039.866622	37.062093
1658.063317	297580.255163	37.067111
1659.666844	298107.452127	37.072128
1661.257365	298667.717964	37.077146
1662.742159	299205.444287	37.082164
1664.441704	299752.453725	37.087181
1665.929100	300313.769222	37.092199
1667.827808	300858.276326	37.097216
1669.402408	301416.218816	37.102234
1670.836015	301984.213677	37.107252
1672.380670	302548.631256	37.112269
1673.672874	303128.249654	37.117287
1675.626366	303693.786801	37.122304
1677.423614	304276.819773	37.127322
1678.869922	304846.548067	37.132340
1680.858701	305415.929380	37.137357
1682.430553	306013.744297	37.142375
1683.987448	306592.433958	37.147392
1685.378941	307177.166137	37.152410
1687.191799	307774.675493	37.157428
1689.113226	308365.382024	37.162445
1691.080807	308955.340380	37.167463
1692.596295	309546.994548	37.172480
1694.426993	310136.408492	37.177498
1696.295848	310732.617935	37.182516
1697.896444	311320.105888	37.187533
1699.317965	311927.884437	37.192551
1701.180809	312516.793273	37.197568
1702.811393	313130.445131	37.202586
1704.255474	313746.383040	37.207604
1705.671156	314350.436146	37.212621
1707.260640	314976.066206	37.217639
1709.410672	315573.843006	37.222656
1710.879041	316200.473171	37.227674
1712.733792	316819.517773	37.232692
1714.612795	317433.271298	37.237709
1716.391346	318052.825784	37.242727
1718.040498	318662.213688	37.247744
1719.562946	319295.968761	37.252762
1721.281103	319912.799833	37.257780
1723.179240	320537.213346	37.262797
1725.147599	321158.562524	37.267815
1727.061962	321766.660419	37.272832
1728.686827	322403.213603	37.277850
1730.693323	323012.148216	37.282868
1732.740614	323620.740355	37.287885
1734.451089	324244.312114	37.292903
1736.315625	324846.245079	37.297920
1737.712088	325474.198424	37.302938
1739.479773	326092.486844	37.307956
1741.155019	326709.083275	37.312973
1742.619434	327342.668527	37.317991
1744.231312	327955.911504	37.323008
1745.898734	328587.647688	37.328026
1747.721094	329222.068264	37.333044
1749.465533	329840.652550	37.338061
1750.978128	330454.038636	37.343079
1752.658701	331046.242445	37.348096
1754.304978	331658.197462	37.353114
1756.034642	332261.221239	37.358132
1758.235707	332858.626477	37.363149
1759.611599	333490.941506	37.368167
1761.544580	334096.730098	37.373184
1763.178999	334720.788687	37.378202
1764.838155	335335.900264	37.383220
1766.788500	335961.415788	37.388237
1768.390121	336578.477513	37.393255
1769.833206	337217.084882	37.398272
1771.641764	337846.231934	37.403290
1773.273201	338472.760732	37.408308
1775.186572	339109.592286	37.413325
1776.565441	339762.699133	37.418343
1778.456219	340411.829581	37.423360
1779.900699	341058.512481	37.428378
1781.728062	341704.387874	37.433396
1783.829666	342364.957016	37.438413
1785.697444	343021.850188	37.443431
1788.271116	343680.471078	37.448448
1789.773056	344320.426824	37.453466
1791.321819	344978.894744	37.458484
1793.489007	345633.876027	37.463501
1795.530997	346286.889347	37.468519
1797.017081	346948.107079	37.473536
1798.706931	347610.677841	37.478554
1799.937780	348276.969608	37.483572
1801.908712	348950.718102	37.488589
1803.766504	349630.058752	37.493607
1805.434921	350304.243395	37.498624
1807.459911	350994.245829	37.503642
1809.374521	351675.449912	37.508660
1811.141948	352347.684395	37.513677
1812.647160	353036.116997	37.518695
1815.114240	353703.064013	37.523712
1817.800524	354385.190327	37.528730
1819.578780	355046.444722	37.533748
1821.113972	355714.859534	37.538765
1823.244777	356387.961522	37.543783
1825.482680	357055.960319	37.548800
1827.643404	357719.368596	37.553818
1829.448241	358395.613411	37.558836
1831.119512	359063.191658	37.563853
1832.693171	359733.439396	37.568871
1834.459437	360393.470115	37.573888
1836.055831	361066.686257	37.578906
1837.569030	361764.718335	37.583924
1839.484435	362430.552157	37.588941
1840.672497	363132.191447	37.593959
1842.232033	363824.522322	37.598976
1844.021336	364512.946957	37.603994
1845.410035	365229.940728	37.609012
1847.439183	365928.803773	37.614029
1849.513468	366645.480742	37.619047
1851.251498	367354.767018	37.624064
1853.175250	368071.087005	37.629082
1855.172174	368794.687083	37.634100
1856.875152	369500.133986	37.639117
1858.615145	370218.269858	37.644135
1860.389713	370935.244712	37.649152
1861.955760	371659.139333	37.654170
1863.584131	372390.289011	37.659188
1865.249202	373123.066634	37.664205
1867.227160	373857.198176	37.669223
1869.293991	374588.510156	37.674240
1871.172637	375322.425186	37.679258
1872.949847	376038.512356	37.684276
1874.759759	376742.203235	37.689293
1876.883047	377470.707350	37.694311
1878.939471	378183.585285	37.699328
1880.695317	378891.350085	37.704346
1882.190319	379623.868703	37.709364
1883.877728	380337.168677	37.714381
1885.644304	381064.615894	37.719399
1887.410802	381804.244522	37.724416
1889.265066	382520.108122	37.729434
1891.014450	383281.716946	37.734452
1892.930708	384022.311375	37.739469
1894.592139	384770.689973	37.744487
1896.500213	385519.416489	37.749504
1898.582101	386264.344707	37.754522
1900.255489	387025.194574	37.759540
1902.941486	387790.777931	37.764557
1904.626380	388538.000814	37.769575
1906.660953	389303.908845	37.774592
1908.587561	390059.143268	37.779610
1910.430105	390830.952725	37.784628
1912.710943	391587.967831	37.789645
1914.463332	392356.534926	37.794663
1916.307924	393129.579767	37.799680
1918.452335	393894.773827	37.804698
1920.180514	394662.628151	37.809716
1922.206239	395439.158625	37.814733
1924.050768	396228.625543	37.819751
1925.810152	397007.035098	37.824768
1927.679515	397798.914988	37.829786
1929.385776	398591.636991	37.834804
1931.561059	399371.107062	37.839821
1933.339600	400183.947591	37.844839
1934.987389	400974.105870	37.849856
1937.266163	401781.522706	37.854874
1938.881940	402582.336333	37.859892
1941.000409	403399.642316	37.864909
1942.597259	404218.075124	37.869927
1944.336030	405045.025269	37.874944
1946.621112	405853.491163	37.879962
1948.541687	406678.234833	37.884980
1950.813855	407506.063098	37.889997
1952.744196	408316.922873	37.895015
1954.874159	409144.396077	37.900032
1956.800265	409954.346781	37.905050
1958.615694	410790.283492	37.910068
1960.726842	411623.257709	37.915085
1962.550456	412452.783132	37.920103
1964.780105	413284.166342	37.925120
1966.764924	414104.950668	37.930138
1968.816161	414947.785691	37.935156
1970.842321	415770.461751	37.940173
1973.419681	416599.859507	37.945191
1975.002361	417431.269082	37.950208
1977.003250	418256.226159	37.955226
1978.619691	419100.669979	37.960244
1980.642766	419933.850857	37.965261
1982.787020	420761.109447	37.970279
1984.160648	421603.788380	37.975296
1986.758258	422432.487511	37.980314
1989.145114	423265.853087	37.985332
1991.680409	424091.342410	37.990349
1993.675428	424905.600963	37.995367
1995.449628	425735.617202	38.000384
1997.823610	426567.025543	38.005402
1999.651732	427387.710691	38.010420
2001.510105	428204.515143	38.015437
2003.287960	429025.305096	38.020455
2004.868149	429827.873446	38.025472
2007.013764	430635.485601	38.030490
2008.745079	431440.354365	38.035508
2010.681557	432246.933823	38.040525
2012.670973	433052.413961	38.045543
2014.355664	433872.900235	38.050560
2016.437351	434683.472367	38.055578
2018.451858	435508.503622	38.060596
2020.200298	436346.810375	38.065613
2022.264778	437158.412308	38.070631
2024.398492	437998.265574	38.075648
2026.649408	438825.517622	38.080666
2028.889756	439660.686628	38.085684
2030.758118	440488.599010	38.090701
2032.905793	441324.733848	38.095719
2034.920081	442171.688208	38.100736
2037.259999	443001.454074	38.105754
2038.992556	443848.998276	38.110772
2040.937076	444701.585187	38.115789
2043.347273	445548.547544	38.120807
2044.698653	446398.586083	38.125824
2046.749798	447246.148940	38.130842
2048.816352	448106.525435	38.135860
2051.239751	448979.202296	38.140877
2052.732911	449835.911530	38.145895
2054.522611	450706.295758	38.150912
2056.698922	451596.964197	38.155930
2058.648223	452480.248340	38.160948
2061.100187	453368.116090	38.165965
2063.205634	454252.918469	38.170983
2065.564909	455133.848692	38.176000
2067.835111	456006.816977	38.181018
2069.411867	456909.697154	38.186036
2071.487810	457800.168288	38.191053
2073.821177	458693.136980	38.196071
2075.901867	459594.956284	38.201088
2077.963615	460489.660600	38.206106
2079.712472	461400.403043	38.211124
2081.565865	462302.189686	38.216141
2083.643776	463225.888381	38.221159
2085.478949	464140.030656	38.226176
2087.898009	465049.990854	38.231194
2090.084562	465969.803563	38.236212
2091.931654	466892.712284	38.241229
2094.527190	467809.642084	38.246247
2096.487737	468747.656758	38.251264
2098.606412	469663.011184	38.256282
2100.903107	470594.665217	38.261300
2103.221688	471518.034204	38.266317
2105.510089	472435.805656	38.271335
2107.476590	473371.875890	38.276352
2109.705172	474295.074642	38.281370
2111.778303	475227.195875	38.286388
2114.076506	476145.644689	38.291405
2116.548512	477059.827068	38.296423
2118.529947	477986.168423	38.301440
2121.203520	478891.438418	38.306458
2123.496536	479810.666793	38.311476
2125.653007	480715.326428	38.316493
2128.205852	481620.128540	38.321511
2130.399958	482526.409426	38.326528
2132.514960	483430.486773	38.331546
2134.931282	484325.834678	38.336564
2136.988499	485226.095040	38.341581
2139.255694	486116.935041	38.346599
2140.911723	487025.198959	38.351616
2143.249867	487920.682934	38.356634
2145.204426	488825.726001	38.361652
2147.084028	489706.252557	38.366669
2149.162284	490578.121199	38.371687
2151.034821	491469.614868	38.376704
2153.080916	492325.249891	38.381722
2155.327454	493220.781378	38.386740
2157.348603	494102.930050	38.391757
2159.505688	494978.753630	38.396775
2161.257252	495874.178460	38.401792
2163.162752	496762.517274	38.406810
2165.268157	497653.753730	38.411828
2167.149244	498567.785349	38.416845
2169.363103	499473.388317	38.421863
2171.083846	500401.120116	38.426880
2173.346035	501333.049608	38.431898
2175.356567	502261.034113	38.436916
2177.172542	503204.534315	38.441933
2179.657138	504156.041279	38.446951
2181.388890	505103.885448	38.451968
2183.115301	506060.349947	38.456986
2185.747887	507020.189526	38.462004
2187.669834	507979.081296	38.467021
2190.152058	508950.933738	38.472039
2192.306273	509931.000132	38.477056
2194.673840	510916.467030	38.482074
2196.843930	511890.966448	38.487092
2199.002735	512871.306212	38.492109
2201.758513	513855.418850	38.497127
2203.490865	514843.318581	38.502144
2205.707189	515838.586305	38.507162
2208.253783	516829.200863	38.512180
2210.359770	517822.697850	38.517197
2213.052583	518823.845309	38.522215
2214.993897	519813.866221	38.527232
2217.228326	520813.902634	38.532250
2219.343708	521821.803547	38.537268
2221.903914	522829.363430	38.542285
2223.996524	523837.286632	38.547303
2225.719554	524850.694468	38.552320
2227.853999	525863.765298	38.557338
2230.435478	526882.486326	38.562356
2232.235230	527915.116392	38.567373
2235.036039	528939.251718	38.572391
2237.291768	529970.053305	38.577408
2239.711130	530986.658455	38.582426
2241.698361	532025.669261	38.587444
2243.830758	533051.443449	38.592461
2246.065359	534082.414812	38.597479
2248.412268	535132.724656	38.602496
2250.645980	536162.592949	38.607514
2252.890318	537195.355832	38.612532
2255.295008	538254.590126	38.617549
2257.337452	539303.238800	38.622567
2259.223769	540356.264533	38.627584
2261.130717	541405.586691	38.632602
2263.455869	542465.881102	38.637620
2265.666003	543537.434124	38.642637
2268.060392	544613.503303	38.647655
2270.060231	545673.761453	38.652672
2272.328162	546737.063764	38.657690
2274.405696	547821.136941	38.662708
2276.430065	548906.542405	38.667725
2279.157474	549986.618012	38.672743
2281.697343	551071.818718	38.677760
2283.670652	552154.211722	38.682778
2286.057796	553241.679105	38.687796
2288.544611	554319.794157	38.692813
2290.879260	555410.414499	38.697831
2293.057111	556480.416797	38.702848
2295.244632	557536.964675	38.707866
2298.090125	558592.366152	38.712884
2299.946854	559643.576356	38.717901
2302.356591	560688.432542	38.722919
2304.765542	561746.369347	38.727936
2307.010785	562799.476183	38.732954
2309.325458	563849.574013	38.737972
2311.198189	564920.856647	38.742989
2313.668041	565971.612751	38.748007
2315.413055	567042.792618	38.753024
2317.924201	568129.525304	38.758042
2320.892083	569201.178851	38.763060
2323.045029	570286.985683	38.768077
2325.001056	571369.520262	38.773095
2327.410741	572450.382542	38.778112
2329.359157	573548.295092	38.783130
2331.943351	574636.823297	38.788148
2334.158703	575749.808943	38.793165
2336.340835	576836.306884	38.798183
2338.982881	577953.643904	38.803200
2340.876474	579077.476714	38.808218
2343.407727	580199.347273	38.813236
2345.602465	581322.225419	38.818253
2347.863773	582446.294836	38.823271
2350.287897	583582.271755	38.828288
2352.263505	584722.831265	38.833306
2354.813683	585876.477924	38.838324
2356.990184	587022.806860	38.843341
2359.289193	588178.182042	38.848359
2361.603664	589350.839356	38.853376
2363.592118	590525.040363	38.858394
2366.214688	591692.606717	38.863412
2368.104090	592875.515173	38.868429
2370.785523	594060.430629	38.873447
2372.866149	595248.734036	38.878464
2375.212157	596434.770158	38.883482
2377.497423	597634.873755	38.888500
2379.629397	598847.752980	38.893517
2381.989067	600058.165031	38.898535
2384.758212	601260.471341	38.903552
2386.970727	602492.739138	38.908570
2389.784535	603704.799162	38.913588
2392.193917	604928.312874	38.918605
2394.747751	606142.261445	38.923623
2397.118080	607360.015476	38.928640
2400.007625	608585.311032	38.933658
2402.755126	609804.392584	38.938676
2405.063514	611022.814622	38.943693
2407.498744	612232.128392	38.948711
2410.008267	613465.161780	38.953728
2412.086831	614677.521961	38.958746
2414.762712	615898.354256	38.963764
2416.843538	617138.203777	38.968781
2419.049929	618357.442165	38.973799
2421.725439	619582.817999	38.978816
2423.641143	620826.229474	38.983834
2426.694913	622059.964456	38.988852
2428.880204	623306.947802	38.993869
2431.071607	624540.043719	38.998887
2433.583420	625779.991900	39.003904
2436.056682	627018.504678	39.008922
2438.518724	628264.220218	39.013940
2440.796956	629525.455944	39.018957
2443.022181	630773.615107	39.023975
2445.444285	632028.087313	39.028992
2448.159348	633292.349305	39.034010
2450.972341	634535.174051	39.039028
2453.412985	635775.916190	39.044045
2455.339204	636997.178491	39.049063
2458.148079	638209.417882	39.054080
2460.126296	639425.096212	39.059098
2462.699103	640649.465735	39.064116
2465.080087	641878.611114	39.069133
2467.768947	643100.025859	39.074151
2470.017494	644328.450708	39.079168
2472.330287	645562.003949	39.084186
2475.104848	646795.281661	39.089204
2477.311103	648041.517273	39.094221
2479.442708	649287.511786	39.099239
2482.423606	650524.388570	39.104256
2484.505900	651780.600636	39.109274
2487.176243	653018.466720	39.114292
2489.772447	654278.017626	39.119309
2492.219143	655546.402002	39.124327
2494.646594	656817.616117	39.129344
2497.338390	658085.733641	39.134362
2500.124665	659347.246920	39.139380
2502.454223	660628.493270	39.144397
2504.837908	661902.840391	39.149415
2507.688293	663169.923650	39.154432
2509.950749	664465.412365	39.159450
2512.454173	665748.045123	39.164468
2514.823211	667046.056295	39.169485
2517.077502	668340.377729	39.174503
2519.928813	669641.540148	39.179520
2522.089191	670958.706722	39.184538
2524.445941	672268.047970	39.189556
2527.219513	673592.954133	39.194573
2529.488459	674905.673876	39.199591
2532.191571	676223.259534	39.204608
2534.765168	677565.685840	39.209626
2537.348961	678881.573905	39.214644
2540.251634	680210.094616	39.219661
2543.127981	681535.497297	39.224679
2546.029813	682874.268789	39.229696
2548.229363	684203.423352	39.234714
2551.028002	685525.779774	39.239732
2553.947737	686864.809525	39.244749
2556.369767	688194.488603	39.249767
2559.127399	689516.222133	39.254784
2561.572844	690855.832865	39.259802
2564.570012	692176.690271	39.264820
2567.140051	693512.856921	39.269837
2569.601464	694832.765858	39.274855
2572.595755	696167.869781	39.279872
2574.926434	697515.481393	39.284890
2577.177753	698834.086346	39.289908
2579.994002	700170.103824	39.294925
2582.337990	701502.178476	39.299943
2585.192373	702844.178404	39.304960
2587.939143	704184.106375	39.309978
2590.554888	705505.860439	39.314996
2593.422494	706843.871571	39.320013
2595.716419	708180.085753	39.325031
2598.361346	709520.988287	39.330048
2600.567692	710864.873896	39.335066
2603.323534	712210.290125	39.340084
2605.694653	713571.450473	39.345101
2608.083699	714905.856484	39.350119
2610.887522	716254.436522	39.355136
2612.839014	717619.321875	39.360154
2615.455688	718973.832073	39.365172
2618.021309	720359.892259	39.370189
2620.211916	721728.917729	39.375207
2622.852338	723099.622327	39.380224
2625.593241	724477.451616	39.385242
2628.135591	725821.614648	39.390260
2630.376670	727167.536102	39.395277
2632.875985	728529.553384	39.400295
2635.622977	729872.427432	39.405312
2638.049694	731238.057726	39.410330
2640.338331	732591.083016	39.415348
2643.321676	733964.956140	39.420365
2645.841523	735323.413683	39.425383
2648.384191	736702.374939	39.430400
2650.845779	738099.969862	39.435418
2652.947669	739473.245586	39.440436
2655.800537	740880.506510	39.445453
2658.333286	742294.330547	39.450471
2660.761553	743703.184176	39.455488
2663.404849	745127.829564	39.460506
2665.790002	746555.465056	39.465524
2668.646015	747994.004197	39.470541
2671.035897	749431.369811	39.475559
2673.730884	750871.377232	39.480576
2676.329740	752336.263694	39.485594
2679.055835	753782.722536	39.490612
2681.895608	755251.106013	39.495629
2684.069805	756726.262645	39.500647
2687.349971	758191.401210	39.505664
2690.282128	759663.257219	39.510682
2693.264619	761139.939079	39.515700
2696.474097	762604.830611	39.520717
2699.190254	764084.476121	39.525735
2701.883958	765563.195409	39.530752
2704.836638	767036.023656	39.535770
2707.707010	768496.873297	39.540788
2710.654782	769976.399973	39.545805
2712.943662	771450.432644	39.550823
2715.731176	772939.126991	39.555840
2718.146691	774422.227393	39.560858
2721.010403	775917.726522	39.565876
2723.809391	777408.020437	39.570893
2726.589333	778916.082738	39.575911
2729.183836	780413.554581	39.580928
2731.702124	781912.497150	39.585946
2734.575608	783432.857851	39.590964
2737.259007	784936.347352	39.595981
2739.716586	786469.136372	39.600999
2742.064297	787980.676133	39.606016
2745.195866	789516.084844	39.611034
2747.810596	791048.061340	39.616052
2750.595924	792567.917167	39.621069
2753.133699	794107.771589	39.626087
2755.538819	795648.389031	39.631104
2758.593176	797209.816565	39.636122
2760.992732	798763.120408	39.641140
2763.930519	800315.353218	39.646157
2766.265184	801881.776631	39.651175
2769.373123	803444.635751	39.656192
2771.893069	805020.495161	39.661210
2774.309205	806598.847408	39.666228
2776.929219	808166.485406	39.671245
2779.724635	809766.732810	39.676263
2782.562225	811367.330290	39.681280
2785.224943	812959.565541	39.686298
2788.424190	814556.711111	39.691316
2791.309209	816140.685082	39.696333
2793.948210	817739.316251	39.701351
2796.728646	819343.302633	39.706368
2799.643208	820944.245758	39.711386
2801.743226	822549.182527	39.716404
2804.861316	824147.270010	39.721421
2807.450206	825762.761060	39.726439
2810.187387	827338.483960	39.731456
2813.027521	828918.295870	39.736474
2815.528961	830500.462086	39.741492
2818.286300	832086.733004	39.746509
2821.096850	833660.868459	39.751527
2823.652752	835250.148951	39.756544
2826.717535	836838.369720	39.761562
2829.087624	838440.914715	39.766580
2832.399433	840034.679831	39.771597
2834.963980	841649.138183	39.776615
2837.807441	843241.983809	39.781632
2840.438004	844856.199841	39.786650
2843.218495	846491.562851	39.791668
2845.927803	848114.849141	39.796685
2848.414684	849756.701364	39.801703
2851.298160	851397.668860	39.806720
2854.077467	853053.469989	39.811738
2856.942763	854712.311287	39.816756
2859.718173	856366.451999	39.821773
2862.677510	858039.819170	39.826791
2865.338331	859704.048703	39.831808
2868.273974	861381.553992	39.836826
2871.133614	863079.943428	39.841844
2874.210565	864761.634717	39.846861
2877.449209	866458.920406	39.851879
2880.207340	868156.487003	39.856896
2883.202544	869863.318755	39.861914
2885.686684	871574.590981	39.866932
2888.605697	873279.300596	39.871949
2891.248100	875003.019793	39.876967
2894.116641	876721.558064	39.881984
2897.478855	878453.056578	39.887002
2900.128951	880180.586952	39.892020
2903.281819	881910.233532	39.897037
2906.001778	883658.090679	39.902055
2909.189604	885391.920061	39.907072
2912.101552	887125.568093	39.912090
2914.848086	888876.103080	39.917108
2917.716041	890627.246077	39.922125
2920.795922	892387.180797	39.927143
2923.521575	894134.770233	39.932160
2926.680620	895897.086025	39.937178
2929.408127	897659.988376	39.942196
2932.329586	899428.864512	39.947213
2935.290332	901202.383501	39.952231
2938.277768	902982.081801	39.957248
2941.561184	904754.621150	39.962266
2944.173568	906522.860332	39.967284
2946.820669	908314.683226	39.972301
2949.234407	910109.718481	39.977319
2952.177917	911903.604407	39.982336
2955.173333	913713.912296	39.987354
2957.616770	915532.555743	39.992372
2960.716778	917349.815592	39.997389
2963.529928	919177.849172	40.002407
2966.290714	921000.478177	40.007424
2969.634241	922841.974576	40.012442
2972.354685	924670.380118	40.017460
2975.384028	926514.416178	40.022477
2978.569384	928342.359610	40.027495
2981.185472	930181.942332	40.032512
2984.193956	932028.393373	40.037530
2987.046193	933883.421351	40.042548
2990.168102	935723.491410	40.047565
2993.175905	937573.656003	40.052583
2995.980666	939424.254976	40.057600
2999.148014	941277.200308	40.062618
3001.837754	943125.073539	40.067636
3005.219065	944946.184304	40.072653
3008.031151	946757.578391	40.077671
3010.876105	948567.758739	40.082688
3014.216672	950376.552503	40.087706
3016.788639	952193.041400	40.092724
3019.847441	954013.001686	40.097741
3022.807532	955858.401246	40.102759
3025.770661	957732.510445	40.107776
3028.762146	959609.331098	40.112794
3031.411932	961486.770320	40.117812
3034.519394	963376.812088	40.122829
3037.502510	965269.965944	40.127847
3040.004391	967182.204303	40.132864
3043.321228	969091.817475	40.137882
3046.019572	971018.951225	40.142900
3049.022601	972948.509288	40.147917
3051.944957	974888.841204	40.152935
3054.927799	976832.015420	40.157952
3057.870484	978788.667420	40.162970
3060.680941	980754.803438	40.167988
3063.775081	982713.593595	40.173005
3066.755246	984699.768315	40.178023
3069.411939	986688.418717	40.183040
3072.757121	988675.969636	40.188058
3075.877993	990685.620385	40.193076
3078.966423	992688.927567	40.198093
3081.943887	994704.957864	40.203111
3085.135876	996729.660113	40.208128
3088.180536	998739.193664	40.213146
3091.127636	1000777.251327	40.218164
3094.242484	1002824.251855	40.223181
3097.336862	1004859.455651	40.228199
3100.182896	1006913.070966	40.233216
3103.534805	1008969.442393	40.238234
3106.645776	1011021.614954	40.243252
3110.078176	1013073.858691	40.248269
3113.420379	1015135.342538	40.253287
3116.669721	1017198.699244	40.258304
3119.654057	1019254.568277	40.263322
3123.006268	1021328.388237	40.268340
3126.099165	1023391.621314	40.273357
3129.629592	1025456.825147	40.278375
3132.385819	1027530.766140	40.283392
3135.920989	1029587.486841	40.288410
3138.760956	1031660.170576	40.293428
3141.994808	1033741.091392	40.298445
3144.906163	1035801.607426	40.303463
3147.499095	1037895.745737	40.308480
3151.184598	1039980.432260	40.313498
3153.945749	1042091.182381	40.318516
3157.009585	1044180.080252	40.323533
3160.367156	1046300.112299	40.328551
3162.874659	1048403.879594	40.333568
3166.342953	1050501.685608	40.338586
3169.762850	1052628.712787	40.343604
3173.050160	1054730.810059	40.348621
3176.209629	1056843.756855	40.353639
3179.168406	1058965.245880	40.358656
3182.427298	1061074.728118	40.363674
3185.785281	1063203.256897	40.368692
3188.753577	1065318.262645	40.373709
3191.892024	1067440.387397	40.378727
3194.977535	1069578.384190	40.383744
3198.349803	1071682.335492	40.388762
3201.433072	1073814.269612	40.393780
3204.688251	1075940.268154	40.398797
3208.078643	1078058.619602	40.403815
3211.171670	1080174.283702	40.408832
3214.368791	1082258.114378	40.413850
3217.387948	1084336.491279	40.418868
3220.509792	1086403.733445	40.423885
3223.769169	1088482.302249	40.428903
3226.695900	1090573.789319	40.433920
3229.826960	1092645.435510	40.438938
3233.241313	1094735.618458	40.443956
3236.351385	1096834.489903	40.448973
3239.869681	1098927.806386	40.453991
3242.405355	1101032.295054	40.459008
3245.526465	1103134.437350	40.464026
3248.656733	1105255.763056	40.469044
3251.703019	1107388.169863	40.474061
3254.896872	1109509.903378	40.479079
3257.816046	1111659.578784	40.484096
3261.375800	1113799.728422	40.489114
3264.288523	1115975.447351	40.494132
3267.123681	1118125.777716	40.499149
3270.892555	1120295.323987	40.504167
3273.640488	1122482.958998	40.509184
3276.974901	1124683.174353	40.514202
3280.009858	1126882.342046	40.519220
3283.368167	1129087.092875	40.524237
3286.647919	1131300.233796	40.529255
3289.410132	1133538.976318	40.534272
3293.154757	1135753.692208	40.539290
3296.614414	1137982.868557	40.544308
3299.733709	1140224.034336	40.549325
3303.212283	1142473.463029	40.554343
3306.559711	1144726.211833	40.559360
3310.146840	1146967.658406	40.564378
3313.405068	1149218.032828	40.569396
3317.308605	1151457.991262	40.574413
3320.518465	1153707.683541	40.579431
3323.525383	1155975.223946	40.584448
3326.887274	1158214.281849	40.589466
3330.159110	1160490.203547	40.594484
3332.898964	1162772.952088	40.599501
3336.644396	1165054.728504	40.604519
3339.423111	1167340.188096	40.609536
3342.723129	1169619.386286	40.614554
3345.844812	1171929.319657	40.619572
3348.797097	1174244.369252	40.624589
3352.161727	1176546.479789	40.629607
3355.314758	1178874.286110	40.634624
3358.821498	1181189.347617	40.639642
3362.161159	1183528.839594	40.644660
3365.545850	1185867.455946	40.649677
3368.994485	1188204.911705	40.654695
3371.980646	1190560.414564	40.659712
3375.085749	1192909.670937	40.664730
3378.533892	1195268.289472	40.669748
3381.689653	1197624.285426	40.674765
3385.093920	1200001.148610	40.679783
3388.111639	1202373.235968	40.684800
3391.600240	1204740.411167	40.689818
3394.935596	1207128.942194	40.694836
3398.284697	1209512.154963	40.699853
3402.038027	1211889.430676	40.704871
3405.121295	1214292.207751	40.709888
3408.506852	1216675.526101	40.714906
3412.028171	1219071.223598	40.719924
3415.418282	1221477.368322	40.724941
3418.646299	1223884.636368	40.729959
3421.772694	1226300.553664	40.734976
3425.019947	1228705.439050	40.739994
3428.645002	1231131.159593	40.745012
3431.961627	1233528.397593	40.750016
3435.504835	1235871.769917	40.755021
3438.600447	1238174.561840	40.760026
3442.164765	1240380.004895	40.765031
3445.575614	1242543.394134	40.770036
3448.381530	1244622.551584	40.775040
3452.020805	1246612.882442	40.780045
3454.834490	1248533.995825	40.785050
3457.842987	1250380.880073	40.790055
3460.534937	1252138.939024	40.795060
3463.260519	1253821.943419	40.800064
3465.812009	1255424.992445	40.805069
3468.108445	1256957.543512	40.810074
3470.809875	1258420.294075	40.815079
3472.935704	1259794.370856	40.820084
3475.376727	1261114.637855	40.825088
3477.709985	1262355.172614	40.830093
3479.198781	1263537.089647	40.835098
3481.532416	1264636.815379	40.840103
3482.749563	1265686.947632	40.845108
3484.961886	1266680.042176	40.850112
3486.815530	1267604.786949	40.855117
3487.958208	1268485.152268	40.860122
3489.926862	1269309.991218	40.865127
3491.688699	1270077.836317	40.870132
3493.049965	1270785.786125	40.875136
3494.408856	1271443.696092	40.880141
3495.558870	1272072.240645	40.885146
3497.368580	1272633.842501	40.890151
3498.151228	1273166.890937	40.895156
3499.427089	1273662.732903	40.900160
3500.991776	1274105.145431	40.905165
3501.769836	1274513.636381	40.910170
3502.461143	1274884.402273	40.915175
3503.671804	1275224.836958	40.920180
3504.811934	1275531.440068	40.925184
3505.640274	1275802.594445	40.930189
3506.389904	1276049.354870	40.935194
3507.277227	1276256.352570	40.940199
3508.336484	1276442.064323	40.945204
3508.696043	1276603.125482	40.950208
3509.262456	1276742.345375	40.955213
3509.898713	1276847.739106	40.960218
3510.202752	1276921.776879	40.965223
3510.979182	1276993.795837	40.970228
3511.702723	1277053.998400	40.975232
3512.301522	1277069.880866	40.980237
3512.359819	1277087.237916	40.985242
3513.271572	1277070.737521	40.990247
3513.651172	1277050.260186	40.995252
3513.805757	1277011.067468	41.000256
3514.304620	1276935.882942	41.005261
3514.614081	1276873.107253	41.010266
3514.834702	1276779.675124	41.015271
3515.423906	1276694.587320	41.020276
3515.785260	1276579.695519	41.025280
3516.038968	1276451.515102	41.030285
3516.233277	1276327.591046	41.035290
3516.640488	1276176.927641	41.040295
3516.682541	1276021.238074	41.045300
3516.869581	1275847.132553	41.050304
3517.427319	1275663.442513	41.055309
3517.544333	1275491.368839	41.060314
3517.789141	1275299.770029	41.065319
3518.420341	1275096.733499	41.070324
3518.202117	1274876.916404	41.075328
3518.393349	1274650.645108	41.080333
3518.539523	1274443.225475	41.085338
3519.078262	1274207.819127	41.090343
3519.084177	1273961.582229	41.095348
3518.771081	1273711.410791	41.100352
3519.342501	1273473.283449	41.105357
3519.169694	1273225.560304	41.110362
3519.224098	1272959.851701	41.115367
3519.946343	1272695.775544	41.120372
3519.712911	1272433.876867	41.125376
3520.047358	1272147.367098	41.130381
3520.147322	1271878.079233	41.135386
3520.160824	1271582.712350	41.140391
3520.624192	1271282.167204	41.145396
3520.020726	1270999.722346	41.150400
3520.481726	1270705.709335	41.155405
3520.444193	1270404.546039	41.160410
3520.700900	1270093.140412	41.165415
3520.954946	1269791.984416	41.170420
3521.061081	1269483.895751	41.175424
3520.722380	1269159.947317	41.180429
3520.745452	1268849.427348	41.185434
3520.725490	1268512.152528	41.190439
3520.869936	1268198.703287	41.195444
3520.855075	1267872.026321	41.200448
3521.109234	1267560.554769	41.205453
3520.850214	1267228.785308	41.210458
3520.980312	1266907.296872	41.215463
3521.112663	1266579.122165	41.220468
3520.757364	1266249.895175	41.225472
3521.322486	1265914.291713	41.230477
3521.230845	1265580.903327	41.235482
3521.011687	1265238.809581	41.240487
3521.205234	1264909.218220	41.245492
3521.368837	1264566.089147	41.250496
3521.607587	1264211.532405	41.255501
3521.307151	1263884.269874	41.260506
3521.186116	1263538.152918	41.265511
3521.195235	1263193.472599	41.270516
3521.234452	1262852.932275	41.275520
3521.256499	1262502.736231	41.280525
3521.143844	1262153.742240	41.285530
3521.186228	1261808.404650	41.290535
3521.306139	1261446.721090	41.295540
3521.176716	1261102.845556	41.300544
3521.198848	1260747.614454	41.305549
3521.364657	1260400.490741	41.310554
3520.875701	1260046.684147	41.315559
3521.280665	1259689.646153	41.320564
3521.006191	1259349.566917	41.325568
3521.207370	1258986.486304	41.330573
3520.860784	1258651.934105	41.335578
3521.031255	1258298.729364	41.340583
3520.894741	1257940.079024	41.345588
3520.598786	1257589.682870	41.350592
3520.692041	1257225.193562	41.355597
3520.755918	1256885.910877	41.360602
3520.997054	1256546.390437	41.365607
3521.047203	1256202.054661	41.370612
3520.524947	1255842.760615	41.375616
3520.792150	1255486.650689	41.380621
3521.124066	1255140.154243	41.385626
3520.968939	1254780.259426	41.390631
3521.181379	1254422.041309	41.395636
3520.897041	1254071.396432	41.400640
3520.611293	1253706.527259	41.405645
3520.725959	1253352.796365	41.410650
3520.736999	1253000.635529	41.415655
3520.601598	1252639.655188	41.420660
3521.076933	1252284.304101	41.425664
3521.278435	1251923.680837	41.430669
3521.148765	1251556.308094	41.435674
3520.948723	1251187.898563	41.440679
3521.030057	1250833.623723	41.445684
3520.603753	1250473.278008	41.450688
3521.017319	1250110.724764	41.455693
3520.543765	1249754.235946	41.460698
3520.724743	1249386.095590	41.465703
3520.843613	1249022.397495	41.470708
3520.705857	1248671.535991	41.475712
3520.678417	1248294.895629	41.480717
3520.337113	1247946.153843	41.485722
3520.508141	1247590.798792	41.490727
3520.621752	1247224.926923	41.495732
3519.808177	1246875.445047	41.500736
3520.669633	1246510.977911	41.505741
3520.545854	1246152.688360	41.510746
3520.482124	1245790.459168	41.515751
3520.604181	1245440.258506	41.520756
3520.233944	1245082.026128	41.525760
3520.856376	1244708.635468	41.530765
3520.352728	1244360.787041	41.535770
3520.581165	1244005.819730	41.540775
3520.503590	1243634.138372	41.545780
3520.340055	1243276.208213	41.550784
3520.435299	1242910.025074	41.555789
3520.021829	1242550.224207	41.560794
3520.083781	1242201.761174	41.565799
3520.169970	1241843.408866	41.570804
3520.017521	1241489.629132	41.575808
3520.046492	1241126.676439	41.580813
3519.996950	1240782.878736	41.585818
3519.585024	1240408.967070	41.590823
3519.760667	1240053.822681	41.595828
3519.806541	1239707.143945	41.600832
3519.848150	1239341.733804	41.605837
3519.561365	1238992.547637	41.610842
3519.404589	1238653.183283	41.615847
3519.608890	1238288.321602	41.620852
3519.361072	1237952.742008	41.625856
3519.708677	1237602.424055	41.630861
3519.673199	1237252.703557	41.635866
3519.267488	1236908.979535	41.640871
3519.655874	1236548.245235	41.645876
3519.454067	1236195.964438	41.650880
3519.371073	1235844.943452	41.655885
3519.196344	1235498.756812	41.660890
3519.281407	1235155.205097	41.665895
3519.340104	1234811.354877	41.670900
3518.900442	1234466.072669	41.675904
3519.209964	1234110.301322	41.680909
3519.017390	1233778.068719	41.685914
3518.908288	1233429.306776	41.690919
3518.591357	1233076.734138	41.695924
3519.029374	1232757.284210	41.700928
3518.821845	1232414.992326	41.705933
3519.036157	1232061.795406	41.710938
3519.132778	1231726.584038	41.715943
3519.306684	1231380.617108	41.720948
3519.131638	1231033.938161	41.725952
3519.022542	1230685.173417	41.730957
3519.203573	1230345.754308	41.735962
3518.820605	1229992.791071	41.740967
3519.166722	1229643.413348	41.745972
3518.556226	1229303.401938	41.750976
3518.716796	1228961.282090	41.755981
3518.590127	1228619.186448	41.760986
3518.816901	1228270.013490	41.765991
3518.579664	1227937.404602	41.770996
3518.396312	1227602.992453	41.776000
3518.503768	1227262.819130	41.781005
3518.550210	1226922.166511	41.786010
3518.184866	1226589.956835	41.791015
3518.315661	1226248.125320	41.796020
3518.039415	1225907.551018	41.801024
3518.281638	1225578.814682	41.806029
3517.895047	1225256.880785	41.811034
3518.091631	1224924.656179	41.816039
3518.007817	1224581.440958	41.821044
3518.014083	1224271.888511	41.826048
3517.888868	1223934.144224	41.831053
3517.949048	1223608.671260	41.836058
3517.715484	1223284.252912	41.841063
3518.317962	1222938.105829	41.846068
3518.144746	1222614.848723	41.851072
3518.172580	1222280.798067	41.856077
3518.062232	1221941.144426	41.861082
3517.874652	1221618.386691	41.866087
3517.931133	1221285.760380	41.871092
3517.591190	1220950.748819	41.876096
3517.562267	1220619.587643	41.881101
3517.902558	1220306.188615	41.886106
3517.800081	1219982.752509	41.891111
3517.893777	1219639.547985	41.896116
3517.509701	1219322.002906	41.901120
3517.434632	1218992.705799	41.906125
3517.332643	1218668.531946	41.911130
3517.304007	1218346.755404	41.916135
3517.502402	1218024.547269	41.921140
3517.310056	1217704.439547	41.926144
3517.309414	1217374.932110	41.931149
3517.367838	1217069.139135	41.936154
3516.920256	1216743.777877	41.941159
3517.493211	1216422.061185	41.946164
3517.324660	1216100.913842	41.951168
3517.426057	1215765.675348	41.956173
3516.999660	1215469.404266	41.961178
3516.901956	1215149.868636	41.966183
3517.104928	1214828.579987	41.971188
3516.775852	1214519.330938	41.976192
3516.880274	1214200.450825	41.981197
3516.913626	1213879.317432	41.986202
3516.852054	1213565.569943	41.991207
3516.675417	1213248.173440	41.996212
3516.953060	1212943.313225	42.001216
3516.728105	1212622.891846	42.006221
3516.755320	1212303.531714	42.011226
3516.587704	1212001.589405	42.016231
3516.650486	1211685.272876	42.021236
3516.485481	1211389.844910	42.026240
3516.395331	1211062.471384	42.031245
3516.577289	1210762.551008	42.036250
3516.322156	1210449.580026	42.041255
3516.595533	1210137.438975	42.046260
3516.328624	1209841.002158	42.051264
3516.537298	1209528.741006	42.056269
3516.124899	1209217.499383	42.061274
3516.600119	1208915.268912	42.066279
3516.539341	1208599.999136	42.071284
3516.102250	1208304.250431	42.076288
3516.448038	1207985.785533	42.081293
3516.312036	1207682.084494	42.086298
3515.862077	1207370.830401	42.091303
3516.087064	1207069.187824	42.096308
3515.657276	1206781.686500	42.101312
3515.963303	1206479.621171	42.106317
3515.984277	1206173.650198	42.111322
3515.659775	1205875.494208	42.116327
3515.747468	1205574.442092	42.121332
3515.867181	1205283.112018	42.126336
3515.927457	1204989.901040	42.131341
3515.663794	1204682.669757	42.136346
3515.429073	1204399.969446	42.141351
3515.808709	1204099.251236	42.146356
3515.566241	1203813.239546	42.151360
3515.528747	1203517.992228	42.156365
3515.545686	1203222.718958	42.161370
3515.333874	1202926.903905	42.166375
3515.709081	1202648.600135	42.171380
3515.027705	1202352.641820	42.176384
3515.452173	1202056.953116	42.181389
3514.764355	1201770.432114	42.186394
3515.170387	1201493.842245	42.191399
3515.258776	1201192.720429	42.196404
3515.119088	1200908.686816	42.201408
3515.300234	1200623.084074	42.206413
3515.169391	1200338.736142	42.211418
3514.987116	1200047.252353	42.216423
3515.318594	1199764.203460	42.221428
3515.094469	1199475.602029	42.226432
3515.308071	1199185.974177	42.231437
3515.087372	1198906.252462	42.236442
3515.082823	1198614.095246	42.241447
3514.674446	1198323.301549	42.246452
3514.584354	1198062.278152	42.251456
3514.943304	1197776.863376	42.256461
3514.535561	1197480.203912	42.261466
3514.478548	1197204.397999	42.266471
3514.661186	1196919.152407	42.271476
3514.429665	1196645.691662	42.276480
3514.472420	1196370.200069	42.281485
3514.547458	1196105.014051	42.286490
3514.640882	1195831.925925	42.291495
3514.432267	1195545.354446	42.296500
3514.153363	1195277.273846	42.301504
3514.290622	1195005.167408	42.306509
3514.462118	1194727.970677	42.311514
3514.201754	1194470.079503	42.316519
3514.302629	1194200.753567	42.321524
3514.271018	1193928.993752	42.326528
3514.143100	1193638.264847	42.331533
3514.351119	1193377.706207	42.336538
3514.201667	1193103.574331	42.341543
3514.103086	1192823.032337	42.346548
3514.293093	1192569.480519	42.351552
3514.184861	1192293.420132	42.356557
3514.256946	1192020.603307	42.361562
3514.120699	1191751.658266	42.366567
3514.209190	1191477.212897	42.371572
3513.897319	1191212.308679	42.376576
3513.988056	1190936.424821	42.381581
3514.137402	1190674.141971	42.386586
3513.824725	1190409.478600	42.391591
3513.915713	1190140.412205	42.396596
3513.592025	1189872.151954	42.401600
3513.692061	1189614.240599	42.406605
3514.100519	1189362.751031	42.411610
3513.869054	1189081.369635	42.416615
3513.954950	1188816.747020	42.421620
3513.555996	1188567.325772	42.426624
3513.502314	1188294.990904	42.431629
3513.600893	1188028.163578	42.436634
3513.663586	1187790.192794	42.441639
3513.824898	1187515.995109	42.446644
3513.277962	1187268.980260	42.451648
3513.305129	1187002.393873	42.456653
3513.333129	1186738.144608	42.461658
3513.296040	1186475.021105	42.466663
3513.408931	1186224.462109	42.471668
3513.314986	1185981.073118	42.476672
3513.244659	1185719.891826	42.481677
3513.218932	1185455.585935	42.486682
3513.117393	1185204.730717	42.491687
3513.339066	1184947.036921	42.496692
3513.278576	1184709.885503	42.501696
3513.198590	1184445.348842	42.506701
3513.147262	1184197.259002	42.511706
3513.092392	1183957.155540	42.516711
3513.046716	1183690.034229	42.521716
3512.835882	1183444.475183	42.526720
3512.764892	1183185.612795	42.531725
3512.771286	1182939.052987	42.536730
3512.717727	1182704.161348	42.541735
3512.953864	1182458.576102	42.546740
3512.574679	1182209.974547	42.551744
3512.707224	1181961.370919	42.556749
3512.961165	1181719.889333	42.561754
3512.800103	1181471.875392	42.566759
3512.866904	1181222.776529	42.571764
3512.572402	1180982.292341	42.576768
3512.682834	1180740.694683	42.581773
3512.651333	1180493.648283	42.586778
3512.403862	1180260.749305	42.591783
3512.795340	1180014.363696	42.596788
3512.219098	1179775.470737	42.601792
3512.320128	1179533.724296	42.606797
3512.560809	1179293.356228	42.611802
3512.496918	1179049.260033	42.616807
3512.427948	1178798.466160	42.621812
3512.490860	1178578.814705	42.626816
3512.274051	1178333.485623	42.631821
3512.360323	1178096.761128	42.636826
3512.281111	1177864.103738	42.641831
3512.418197	1177616.798526	42.646836
3512.290131	1177373.105186	42.651840
3512.133001	1177137.790253	42.656845
3512.197611	1176909.023415	42.661850
3511.841892	1176674.285518	42.666855
3511.935286	1176441.818718	42.671860
3512.069345	1176221.019429	42.676864
3512.181111	1175987.869708	42.681869
3512.444324	1175742.150807	42.686874
3511.957000	1175515.109872	42.691879
3512.318216	1175277.929045	42.696884
3511.863532	1175053.124516	42.701888
3511.984596	1174818.318591	42.706893
3511.946174	1174590.597849	42.711898
3511.675951	1174354.892865	42.716903
3511.958036	1174113.618669	42.721908
3511.874538	1173885.497440	42.726912
3511.813512	1173650.480299	42.731917
3511.949579	1173442.667313	42.736922
3511.508764	1173219.101220	42.741927
3512.015336	1172977.266002	42.746932
3511.771786	1172751.855873	42.751936
3511.749283	1172529.134209	42.756941
3511.717166	1172300.369321	42.761946
3511.557633	1172070.012181	42.766951
3511.837328	1171837.592017	42.771956
3511.766643	1171624.081973	42.776960
3511.417299	1171377.409194	42.781965
3511.560312	1171158.091464	42.786970
3511.401477	1170940.417768	42.791975
3511.757107	1170710.387344	42.796980
3511.724477	1170493.523187	42.801985
3511.264836	1170265.777115	42.806989
3511.633192	1170040.998028	42.811994
3511.482396	1169825.540702	42.816999
3511.499754	1169595.422498	42.822004
3511.102326	1169373.193882	42.827009
3511.126354	1169148.999220	42.832013
3511.159984	1168934.135227	42.837018
3511.274546	1168727.175821	42.842023
3511.130319	1168507.982744	42.847028
3511.006043	1168295.855224	42.852033
3511.168105	1168082.350642	42.857037
3511.490599	1167856.069384	42.862042
3511.115307	1167629.421322	42.867047
3511.349948	1167419.464362	42.872052
3511.013501	1167202.985475	42.877057
3510.955785	1166988.150865	42.882061
3510.952373	1166772.165664	42.887066
3510.836205	1166563.459310	42.892071
3511.081932	1166351.097480	42.897076
3510.335592	1166148.520512	42.902081
3510.500261	1165936.627260	42.907085
3510.976315	1165732.511019	42.912090
3510.357146	1165529.605855	42.917095
3510.749983	1165321.049344	42.922100
3510.634222	1165108.130010	42.927105
3510.384702	1164887.858081	42.932109
3510.494291	1164697.266052	42.937114
3510.688431	1164493.714549	42.942119
3510.524484	1164284.452883	42.947124
3510.242792	1164076.618990	42.952129
3510.532451	1163877.183578	42.957133
3510.578745	1163689.587794	42.962138
3510.513122	1163468.092321	42.967143
3510.622996	1163250.242707	42.972148
3510.438755	1163067.480310	42.977153
3510.250558	1162859.960578	42.982157
3510.318732	1162665.711461	42.987162
3510.237502	1162456.741001	42.992167
3510.156110	1162249.651890	42.997172
3510.334960	1162066.322336	43.002177
3510.223681	1161868.860689	43.007181
3510.688678	1161667.422459	43.012186
3510.125707	1161468.035732	43.017191
3510.239836	1161253.882270	43.022196
3510.267110	1161068.936273	43.027201
3509.910230	1160866.752094	43.032205
3510.327733	1160667.267922	43.037210
3510.133843	1160475.249033	43.042215
3510.194496	1160275.714225	43.047220
3510.116773	1160084.985170	43.052225
3510.015416	1159883.288105	43.057229
3510.004621	1159686.672946	43.062234
3509.957641	1159499.415111	43.067239
3509.888273	1159303.551498	43.072244
3509.919652	1159103.882393	43.077249
3509.799573	1158905.365154	43.082253
3510.084720	1158731.733978	43.087258
3509.630701	1158530.515706	43.092263
3509.720841	1158341.586611	43.097268
3509.953490	1158149.034084	43.102273
3509.991717	1157961.234534	43.107277
3510.113620	1157763.107034	43.112282
3509.487000	1157579.374999	43.117287
3509.726379	1157380.551745	43.122292
3509.769550	1157205.869681	43.127297
3509.627731	1157016.741965	43.132301
3509.742290	1156821.890367	43.137306
3509.483646	1156635.416421	43.142311
3509.553946	1156449.070853	43.147316
3509.899874	1156264.470508	43.152321
3509.424293	1156067.796316	43.157325
3509.677543	1155890.481862	43.162330
3509.418975	1155697.352766	43.167335
3509.717394	1155511.787800	43.172340
3509.465201	1155340.403504	43.177345
3509.460810	1155151.753652	43.182349
3509.655405	1154952.088992	43.187354
3509.247743	1154775.508080	43.192359
3509.543216	1154586.883192	43.197364
3509.225353	1154414.249437	43.202369
3509.033447	1154225.124097	43.207373
3509.445592	1154051.411925	43.212378
3509.026060	1153876.790022	43.217383
3509.619711	1153679.944991	43.222388
3508.779848	1153510.206643	43.227393
3508.885433	1153340.401743	43.232397
3509.274419	1153149.438471	43.237402
3508.719815	1152984.841758	43.242407
3509.020921	1152802.398850	43.247412
3508.963092	1152644.997975	43.252417
3508.735687	1152471.717616	43.257421
3508.961199	1152286.050856	43.262426
3508.560864	1152111.461841	43.267431
3509.053867	1151930.377098	43.272436
3508.852397	1151777.991399	43.277441
3508.752084	1151602.200022	43.282445
3509.046966	1151422.645251	43.287450
3508.852102	1151256.325688	43.292455
3508.819418	1151080.127022	43.297460
3509.219769	1150911.520808	43.302465
3508.841234	1150741.522437	43.307469
3508.995328	1150561.677441	43.312474
3508.788301	1150395.143299	43.317479
3508.648610	1150214.577270	43.322484
3508.844848	1150042.188873	43.327489
3508.751296	1149877.419030	43.332493
3508.867969	1149711.094073	43.337498
3508.640142	1149547.946092	43.342503
3508.887135	1149368.329211	43.347508
3508.751204	1149201.366771	43.352513
3508.554933	1149042.744411	43.357517
3508.622296	1148863.139906	43.362522
3508.620851	1148697.181313	43.367527
3508.979165	1148526.516479	43.372532
3508.642476	1148356.907921	43.377537
3508.827764	1148185.407952	43.382541
3509.026261	1148013.521277	43.387546
3508.717289	1147856.871327	43.392551
3508.777307	1147684.144050	43.397556
3508.622400	1147504.719388	43.402561
3508.532373	1147341.480432	43.407565
3508.815275	1147183.670747	43.412570
3508.471108	1147018.852846	43.417575
3509.001369	1146836.260385	43.422580
3508.633215	1146671.151294	43.427585
3508.424164	1146495.586530	43.432589
3508.465294	1146327.271978	43.437594
3508.365848	1146174.707425	43.442599
3508.270867	1146009.816969	43.447604
3508.298612	1145855.895403	43.452609
3508.424076	1145678.542371	43.457613
3508.632655	1145522.780475	43.462618
3508.263044	1145354.976499	43.467623
3508.473302	1145195.034036	43.472628
3508.645342	1145042.297266	43.477633
3508.116072	1144863.223634	43.482637
3508.004608	1144705.973634	43.487642
3508.105431	1144544.038719	43.492647
3507.969159	1144394.936469	43.497652
3508.101468	1144237.632382	43.502657
3507.891404	1144090.429832	43.507661
3507.996376	1143928.096124	43.512666
3507.995693	1143777.342305	43.517671
3508.096290	1143615.094523	43.522676
3508.079326	1143461.205371	43.527681
3507.904637	1143306.199832	43.532685
3507.893233	1143155.335219	43.537690
3508.105020	1143004.524372	43.542695
3508.053104	1142836.208745	43.547700
3508.154397	1142690.243572	43.552705
3507.995090	1142544.317291	43.557709
3508.065305	1142391.141340	43.562714
3507.559713	1142229.519925	43.567719
3507.724771	1142080.492448	43.572724
3507.728184	1141930.728611	43.577729
3507.610203	1141780.411421	43.582733
3507.747069	1141632.229624	43.587738
3507.551629	1141486.754386	43.592743
3507.651627	1141336.862978	43.597748
3507.851879	1141186.191921	43.602753
3507.565746	1141042.711507	43.607757
3507.642877	1140888.542278	43.612762
3507.656938	1140743.581308	43.617767
3507.582858	1140603.943728	43.622772
3507.492362	1140459.087061	43.627777
3507.527308	1140298.835623	43.632781
3507.420490	1140148.944644	43.637786
3507.396757	1140012.509102	43.642791
3507.421088	1139872.266720	43.647796
3507.289301	1139734.038980	43.652801
3507.052732	1139593.642415	43.657805
3507.274468	1139459.809132	43.662810
3507.135129	1139315.688372	43.667815
3507.224084	1139173.044455	43.672820
3507.270090	1139032.017077	43.677825
3507.080328	1138888.082788	43.682829
3507.019056	1138750.956614	43.687834
3507.201059	1138619.101657	43.692839
3507.142640	1138477.981826	43.697844
3507.626104	1138353.188868	43.702849
3507.226914	1138198.165564	43.707853
3507.304695	1138052.171287	43.712858
3506.943934	1137934.436512	43.717863
3507.228326	1137783.844659	43.722868
3506.922282	1137654.514080	43.727873
3507.187565	1137521.099301	43.732877
3507.139124	1137380.233384	43.737882
3506.926697	1137241.858974	43.742887
3507.177812	1137098.183192	43.747892
3506.957237	1136978.695268	43.752897
3506.810508	1136843.812320	43.757901
3507.228211	1136703.516233	43.762906
3506.825718	1136576.074067	43.767911
3507.293215	1136434.908181	43.772916
3507.011841	1136299.273987	43.777921
3506.948596	1136169.392445	43.782925
3507.137556	1136033.863905	43.787930
3506.777650	1135902.410469	43.792935
3506.813316	1135770.508789	43.797940
3506.682237	1135645.278561	43.802945
3506.753302	1135511.750285	43.807949
3506.844163	1135373.087242	43.812954
3506.705798	1135254.971432	43.817959
3506.700670	1135117.172224	43.822964
3506.909634	1135004.976777	43.827969
3506.386057	1134873.904701	43.832973
3506.790600	1134738.497535	43.837978
3506.552714	1134620.383996	43.842983
3506.795605	1134491.455741	43.847988
3506.936091	1134360.356596	43.852993
3506.935471	1134220.633700	43.857997
3506.741359	1134102.596419	43.863002
3506.461364	1133971.746910	43.868007
3506.464678	1133833.913008	43.873012
3506.692422	1133720.737410	43.878017
3506.476760	1133585.308006	43.883021
3506.554035	1133456.761910	43.888026
3506.551310	1133330.695942	43.893031
3506.403564	1133204.555862	43.898036
3506.496206	1133084.453628	43.903041
3506.321604	1132972.183415	43.908045
3506.818711	1132847.638815	43.913050
3506.224528	1132729.351870	43.918055
3506.584811	1132611.285153	43.923060
3506.746599	1132472.439683	43.928065
3506.415657	1132346.499441	43.933069
3506.330986	1132216.049611	43.938074
3506.018219	1132106.729555	43.943079
3506.063951	1131988.035637	43.948084
3506.317820	1131865.693708	43.953089
3506.113137	1131750.266693	43.958093
3506.529236	1131625.801857	43.963098
3505.934941	1131508.343035	43.968103
3506.017338	1131385.448092	43.973108
3506.108785	1131283.837573	43.978113
3506.214833	1131167.301298	43.983117
3506.491091	1131046.362455	43.988122
3506.003998	1130938.852910	43.993127
3506.264461	1130810.117599	43.998132
3506.152367	1130693.416777	44.003137
3505.924032	1130584.716860	44.008141
3505.992592	1130470.357674	44.013146
3505.992117	1130351.349681	44.018151
3506.015190	1130245.072861	44.023156
3505.883576	1130128.838156	44.028161
3505.675993	1130015.845515	44.033165
3506.171874	1129899.692582	44.038170
3506.050950	1129790.483428	44.043175
3505.897289	1129679.851411	44.048180
3506.000386	1129572.692378	44.053185
3506.006618	1129453.663207	44.058189
3506.165220	1129334.035838	44.063194
3506.065887	1129233.653551	44.068199
3505.904173	1129110.365966	44.073204
3505.936816	1128996.456418	44.078209
3505.348942	1128893.485942	44.083213
3505.805360	1128788.059477	44.088218
3505.844229	1128680.417648	44.093223
3505.834041	1128558.138258	44.098228
3505.806924	1128452.024082	44.103233
3505.475044	1128346.813807	44.108237
3505.658447	1128244.559568	44.113242
3505.382555	1128133.344981	44.118247
3505.801334	1128027.053806	44.123252
3505.565958	1127922.484932	44.128257
3505.616828	1127818.247263	44.133261
3506.033092	1127703.010561	44.138266
3505.603464	1127610.165184	44.143271
3505.590488	1127493.092548	44.148276
3505.781966	1127384.163006	44.153281
3505.207272	1127301.132300	44.158285
3505.389833	1127176.601920	44.163290
3505.503483	1127071.768637	44.168295
3505.442617	1126970.671556	44.173300
3505.449735	1126861.095878	44.178305
3505.261443	1126766.959518	44.183309
3505.746420	1126661.105808	44.188314
3505.432160	1126559.947549	44.193319
3505.550538	1126462.996739	44.198324
3505.317757	1126362.677439	44.203329
3505.105342	1126261.591868	44.208333
3505.310339	1126158.342764	44.213338
3505.196283	1126075.692734	44.218343
3505.198188	1125961.913628	44.223348
3505.337647	1125853.627321	44.228353
3504.965466	1125771.871315	44.233357
3505.632513	1125668.822051	44.238362
3505.535642	1125565.040347	44.243367
3505.376829	1125456.985395	44.248372
3505.422892	1125368.208878	44.253377
3505.224614	1125267.292414	44.258381
3505.451775	1125171.346818	44.263386
3505.207654	1125074.145020	44.268391
3505.252092	1124974.419987	44.273396
3505.356083	1124880.297323	44.278401
3505.027796	1124772.922495	44.283405
3504.964812	1124678.633463	44.288410
3505.117822	1124594.298821	44.293415
3504.932778	1124499.170296	44.298420
3505.051447	1124400.469070	44.303425
3505.035937	1124311.114133	44.308429
3504.857283	1124221.023251	44.313434
3505.229072	1124127.699693	44.318439
3505.051119	1124035.892571	44.323444
3505.224963	1123948.118232	44.328449
3504.795666	1123849.877752	44.333453
3505.015358	1123747.911989	44.338458
3505.240956	1123665.454187	44.343463
3505.149350	1123574.957362	44.348468
3505.071006	1123474.177575	44.353473
3504.823458	1123397.218715	44.358477
3505.101727	1123289.904498	44.363482
3504.991745	1123191.599308	44.368487
3504.903212	1123107.566513	44.373492
3505.262078	1123020.412748	44.378497
3505.150678	1122909.537985	44.383501
3505.186785	1122809.678690	44.388506
3504.901062	1122735.286705	44.393511
3504.885615	1122639.621142	44.398516
3504.847724	1122548.526912	44.403521
3504.692861	1122461.639033	44.408525
3504.712844	1122379.671230	44.413530
3504.968510	1122298.424946	44.418535
3504.731714	1122200.598393	44.423540
3504.729733	1122106.444277	44.428545
3504.728340	1122027.425871	44.433549
3504.739878	1121930.124688	44.438554
3504.763447	1121855.479092	44.443559
3504.862914	1121755.780075	44.448564
3505.020754	1121669.684692	44.453569
3504.557071	1121591.497660	44.458573
3504.736990	1121493.208671	44.463578
3505.153843	1121416.968761	44.468583
3504.611006	1121327.555528	44.473588
3504.673061	1121243.659038	44.478593
3504.697993	1121161.386077	44.483597
3505.108575	1121073.715958	44.488602
3504.744995	1120984.172232	44.493607
3504.652912	1120889.821075	44.498612
3504.794766	1120795.239271	44.503617
3504.517877	1120718.913218	44.508621
3504.915071	1120634.190148	44.513626
3504.460760	1120559.795620	44.518631
3504.606561	1120460.540965	44.523636
3505.025789	1120377.429145	44.528641
3504.591217	1120303.218259	44.533645
3504.919207	1120213.452482	44.538650
3504.463301	1120123.814305	44.543655
3504.383408	1120037.160360	44.548660
3504.893762	1119952.693582	44.553665
3504.639605	1119869.399054	44.558669
3504.668891	1119773.008105	44.563674
3504.425393	1119703.329137	44.568679
3504.928822	1119608.095318	44.573684
3505.170707	1119535.953050	44.578689
3504.292582	1119446.944548	44.583693
3504.359221	1119358.064715	44.588698
3504.288694	1119282.731931	44.593703
3504.468726	1119199.641217	44.598708
3504.322490	1119118.984346	44.603713
3504.506551	1119032.080132	44.608717
3504.820948	1118945.248301	44.613722
3504.155492	1118875.151740	44.618727
3504.419677	1118798.328106	44.623732
3504.164097	1118716.540036	44.628737
3504.392417	1118646.960121	44.633741
3504.617413	1118571.949714	44.638746
3504.139872	1118497.435030	44.643751
3504.419160	1118416.697488	44.648756
3504.307271	1118339.929216	44.653761
3504.016948	1118269.572388	44.658765
3504.345798	1118193.872683	44.663770
3504.323497	1118117.753374	44.668775
3504.426589	1118027.606884	44.673780
3504.335791	1117941.778268	44.678785
3504.238978	1117870.622108	44.683789
3504.345358	1117793.810053	44.688794
3504.455438	1117731.669511	44.693799
3503.982827	1117646.089598	44.698804
3504.469327	1117571.593802	44.703809
3503.935608	1117504.030211	44.708813
3504.285462	1117419.073485	44.713818
3503.990590	1117352.993226	44.718823
3504.186368	1117284.639706	44.723828
3504.363784	1117200.279643	44.728833
3504.034011	1117133.440101	44.733837
3503.880488	1117045.511038	44.738842
3503.879926	1116975.375346	44.743847
3504.156198	1116909.672017	44.748852
3504.327996	1116838.076713	44.753857
3504.031915	1116758.457201	44.758861
3504.379488	1116683.495456	44.763866
3504.583913	1116624.280804	44.768871
3504.357697	1116539.214408	44.773876
3504.604312	1116468.078348	44.778881
3504.326675	1116388.640905	44.783885
3504.594674	1116290.337131	44.788890
3504.273244	1116215.764949	44.793895
3503.934729	1116148.438008	44.798900
3503.974919	1116070.849677	44.803905
3504.206722	1116000.567644	44.808909
3504.350956	1115928.869423	44.813914
3503.816819	1115854.422552	44.818919
3504.087507	1115777.554525	44.823924
3504.162581	1115709.582057	44.828929
3504.141760	1115649.535886	44.833933
3504.295650	1115561.245873	44.838938
3504.071736	1115504.091095	44.843943
3503.879500	1115418.238736	44.848948
3504.164877	1115350.513044	44.853953
3504.040727	1115284.474455	44.858957
3503.932538	1115203.085036	44.863962
3504.026569	1115136.150755	44.868967
3503.837520	1115066.402424	44.873972
3504.280774	1114996.263058	44.878977
3503.871932	1114918.732005	44.883981
3503.641713	1114848.892293	44.888986
3504.102459	1114787.899170	44.893991
3503.702194	1114715.035066	44.898996
3503.664054	1114649.832498	44.904001
3503.943595	1114594.873150	44.909005
3504.167228	1114511.130502	44.914010
3503.740459	1114444.082682	44.919015
3503.813172	1114385.246351	44.924020
3503.597647	1114314.729877	44.929025
3503.843320	1114253.194053	44.934029
3504.230765	1114182.576534	44.939034
3503.839457	1114111.514277	44.944039
3503.653465	1114039.749838	44.949044
3504.009522	1113982.674002	44.954049
3504.017055	1113908.778299	44.959053
3504.203106	1113831.610279	44.964058
3503.785683	1113774.278220	44.969063
3503.835010	1113704.758962	44.974068
3503.919709	1113642.479832	44.979073
3503.599884	1113574.640692	44.984077
3503.772819	1113517.017940	44.989082
3503.823911	1113447.113632	44.994087
3503.636930	1113383.064457	44.999092
3503.763780	1113309.903715	45.004097
3503.591624	1113246.613342	45.009101
3503.464382	1113182.647295	45.014106
3503.854976	1113126.224199	45.019111
3503.829064	1113056.232119	45.024116
3504.048039	1112992.302145	45.029121
3503.870380	1112927.864540	45.034125
3503.875142	1112849.663235	45.039130
3504.125711	1112796.406859	45.044135
3503.990638	1112737.109835	45.049140
3503.990401	1112668.443639	45.054145
3503.890184	1112597.217993	45.059149
3503.735753	1112521.136300	45.064154
3503.668208	1112456.007279	45.069159
3503.474219	1112393.091928	45.074164
3503.766004	1112318.269124	45.079169
3503.570056	1112265.844042	45.084173
3504.114491	1112202.327950	45.089178
3503.836848	1112131.411480	45.094183
3503.551156	1112067.458234	45.099188
3503.654435	1112021.181257	45.104193
3503.638139	1111956.896178	45.109197
3503.752849	1111876.945695	45.114202
3503.730736	1111825.727683	45.119207
3503.363434	1111757.873378	45.124212
3503.784224	1111690.365357	45.129217
3503.759071	1111635.902843	45.134221
3503.981538	1111565.373470	45.139226
3503.651163	1111503.710227	45.144231
3503.485589	1111442.877664	45.149236
3503.734969	1111377.683362	45.154241
3503.351283	1111317.648451	45.159245
3503.392112	1111255.444245	45.164250
3503.471387	1111196.476476	45.169255
3503.430308	1111140.962202	45.174260
3503.604617	1111090.086413	45.179265
3503.331690	1111029.362243	45.184269
3503.447263	1110959.224117	45.189274
3503.589577	1110907.111654	45.194279
3503.262591	1110846.203512	45.199284
3503.737114	1110785.258074	45.204289
3503.209384	1110736.116428	45.209293
3503.469446	1110677.303996	45.214298
3503.512206	1110616.427756	45.219303
3503.376017	1110551.954790	45.224308
3503.532691	1110491.821643	45.229313
3503.215845	1110445.314057	45.234317
3503.605727	1110376.554299	45.239322
3503.568783	1110321.317106	45.244327
3503.707414	1110265.955015	45.249332
3503.586609	1110204.337740	45.254337
3503.131403	1110154.224674	45.259341
3503.309875	1110092.461410	45.264346
3503.272563	1110037.125939	45.269351
3502.922611	1109980.600952	45.274356
3503.399817	1109931.286420	45.279361
3503.295970	1109877.009870	45.284365
3503.396087	1109821.458705	45.289370
3503.284656	1109776.056543	45.294375
3503.447039	1109713.814469	45.299380
3503.394009	1109646.645095	45.304385
3503.478534	1109610.465405	45.309389
3503.496594	1109540.897378	45.314394
3503.665130	1109484.377201	45.319399
3503.342462	1109433.281302	45.324404
3503.398725	1109366.662997	45.329409
3503.232871	1109307.237724	45.334413
3503.468855	1109246.314142	45.339418
3503.545416	1109197.345167	45.344423
3503.311168	1109128.385951	45.349428
3503.805128	1109076.579561	45.354433
3503.268481	1109021.983919	45.359437
3503.353259	1108963.181610	45.364442
3503.548317	1108902.451747	45.369447
3503.557992	1108857.689942	45.374452
3503.774540	1108797.432546	45.379457
3503.325455	1108738.047627	45.384461
3503.570761	1108676.734298	45.389466
3503.680491	1108626.895694	45.394471
3503.384247	1108552.117308	45.399476
3503.678829	1108493.657087	45.404481
3503.493501	1108451.310133	45.409485
3503.527614	1108367.884676	45.414490
3503.277596	1108324.783805	45.419495
3502.967828	1108271.479431	45.424500
3503.370981	1108212.043783	45.429505
3503.322628	1108157.740731	45.434509
3503.455401	1108096.534776	45.439514
3503.571727	1108047.166974	45.444519
3503.287555	1107987.460238	45.449524
3503.364972	1107930.652382	45.454529
3503.362700	1107880.443491	45.459533
3503.271369	1107829.771516	45.464538
3503.270423	1107772.974901	45.469543
3503.168239	1107715.526151	45.474548
3503.412894	1107657.160528	45.479553
3503.138815	1107621.408358	45.484557
3503.105743	1107559.650850	45.489562
3503.186589	1107504.842620	45.494567
3502.914258	1107465.461558	45.499572
3503.300660	1107402.296676	45.504577
3503.220453	1107345.890464	45.509581
3503.391473	1107295.743040	45.514586
3502.852303	1107246.284918	45.519591
3503.028981	1107197.376715	45.524596
3502.920225	1107142.691492	45.529601
3502.795628	1107104.810954	45.534605
3502.921429	1107044.357936	45.539610
3503.158241	1107008.994901	45.544615
3502.714449	1106955.985968	45.549620
3502.662606	1106900.429661	45.554625
3502.714104	1106864.905255	45.559629
3503.091467	1106821.975423	45.564634
3502.930671	1106764.048793	45.569639
3502.930931	1106733.878581	45.574644
3503.278765	1106674.530554	45.579649
3502.825410	1106628.489782	45.584653
3502.935950	1106581.019040	45.589658
3503.099101	1106535.926202	45.594663
3502.871946	1106486.314217	45.599668
3503.255625	1106443.953217	45.604673
3503.478721	1106395.030083	45.609677
3503.251378	1106330.330522	45.614682
3503.184368	1106283.363815	45.619687
3502.892664	1106238.343400	45.624692
3503.124781	1106179.677374	45.629697
3502.859233	1106136.561514	45.634701
3503.099735	1106089.065032	45.639706
3503.256335	1106038.526327	45.644711
3503.057891	1105980.406485	45.649716
3503.018367	1105941.835322	45.654721
3502.929064	1105890.380827	45.659725
3503.144619	1105838.493663	45.664730
3503.021655	1105803.372955	45.669735
3502.850918	1105757.564653	45.674740
3502.956793	1105700.155610	45.679745
3503.053401	1105659.077149	45.684749
3503.186808	1105604.431906	45.689754
3502.867422	1105558.837387	45.694759
3502.537468	1105525.658892	45.699764
3503.090531	1105463.112309	45.704769
3502.807020	1105425.628116	45.709773
3502.859122	1105374.145398	45.714778
3503.032795	1105326.844206	45.719783
3502.830808	1105275.402392	45.724788
3502.898573	1105232.892906	45.729793
3502.872881	1105199.853294	45.734797
3503.077579	1105152.640967	45.739802
3503.046976	1105098.590629	45.744807
3502.673509	1105050.231063	45.749812
3503.171834	1104996.379104	45.754817
3502.964512	1104938.631502	45.759821
3503.181447	1104833.631858	45.764826
3503.238829	1104656.735818	45.769831
3503.097304	1104425.708946	45.774836
3502.794542	1104126.973943	45.779841
3502.679439	1103794.756757	45.784845
3502.790601	1103369.908658	45.789850
3502.613083	1102897.111780	45.794855
3502.051553	1102367.100546	45.799860
3502.536669	1101753.724618	45.804865
3502.398084	1101093.740868	45.809869
3502.472162	1100356.501656	45.814874
3502.175594	1099554.882296	45.819879
3502.056319	1098686.755914	45.824884
3501.964241	1097733.275125	45.829889
3501.580660	1096721.421633	45.834893
3501.732528	1095619.741667	45.839898
3501.652128	1094465.436068	45.844903
3501.016817	1093235.552944	45.849908
3501.044511	1091926.968229	45.854913
3500.712867	1090537.878381	45.859917
3500.517203	1089059.519251	45.864922
3500.427645	1087524.400622	45.869927
3500.104840	1085890.742655	45.874932
3500.025260	1084178.320443	45.879937
3499.473192	1082409.044666	45.884941
3499.424156	1080531.660548	45.889946
3499.496428	1078578.079233	45.894951
3499.029581	1076546.312307	45.899956
3499.099093	1074429.180885	45.904961
3498.552437	1072223.413792	45.909965
3498.150200	1069931.951769	45.914970
3497.753345	1067573.175547	45.919975
3497.170620	1065121.632014	45.924980
3497.152553	1062585.641486	45.929985
3496.516410	1059972.795216	45.934989
3496.080433	1057282.658147	45.939994
3495.396567	1054514.614751	45.944999
3494.919870	1051656.708887	45.950004
3494.807120	1048720.550485	45.955009
3494.116425	1045705.979941	45.960013
3493.633219	1042598.445627	45.965018
3493.163365	1039414.161971	45.970023
3492.371236	1036163.694565	45.975028
3492.206912	1032814.452701	45.980033
3491.624349	1029394.032190	45.985037
3490.627098	1025885.640410	45.990042
3490.532712	1022295.880198	45.995047
3489.482590	1018632.668141	46.000052
3488.835585	1014881.855907	46.005057
3488.321222	1011049.147584	46.010061
3487.626515	1007124.906472	46.015066
3487.132961	1003132.331176	46.020071
3486.638987	999061.678945	46.025076
3486.150890	994887.066933	46.030081
3485.183782	990651.448589	46.035085
3484.372372	986321.903837	46.040090
3484.091209	981917.695567	46.045095
3483.270768	977428.770731	46.050100
3482.659557	972838.678301	46.055105
3481.892148	968175.142851	46.060109
3481.189271	963431.592214	46.065114
3480.188995	958604.664029	46.070119
3479.213227	953710.335392	46.075124
3478.538075	948842.431888	46.080129
3477.714548	943895.488953	46.085133
3476.631603	938848.533535	46.090138
3475.824968	933739.641434	46.095143
3474.635185	928555.148202	46.100148
3474.413611	923281.678957	46.105153
3472.926425	917910.153966	46.110157
3471.639449	912468.148797	46.115162
3470.909702	906959.799143	46.120167
3469.874417	901361.935423	46.125172
3468.760666	895676.929062	46.130177
3467.396330	889906.454427	46.135181
3466.461231	884059.609886	46.140186
3465.597189	878140.564805	46.145191
3464.555944	872129.125957	46.150196
3462.834136	866042.373326	46.155201
3461.512220	859879.593003	46.160205
3460.538785	853615.723109	46.165210
3459.486724	847296.712538	46.170215
3458.001176	840890.153089	46.175220
3456.968498	834395.188378	46.180225
3455.650597	827821.005514	46.185229
3454.270141	821165.762650	46.190234
3452.926890	814440.025339	46.195239
3451.531936	807629.874563	46.200244
3450.622526	800731.394289	46.205249
3449.054161	793751.692195	46.210253
3447.575394	786689.433246	46.215258
3446.295532	779556.676705	46.220263
3444.824385	772346.253153	46.225268
3443.286308	765030.466668	46.230273
3441.746998	757652.515291	46.235277
3440.238418	750194.997148	46.240282
3438.726124	742663.408258	46.245287
3437.495639	735041.830348	46.250292
3435.600578	727340.409905	46.255297
3434.111272	719557.149691	46.260301
3432.871432	711700.232203	46.265306
3431.254129	703765.778281	46.270311
3429.231714	695756.565153	46.275316
3427.682584	687660.450791	46.280321
3426.020544	679493.849023	46.285325
3424.213906	671257.785885	46.290330
3422.699206	662928.112305	46.295335
3420.738173	654530.453279	46.300340
3419.149421	646063.371228	46.305345
3416.809543	637528.301879	46.310349
3415.178927	628900.573237	46.315354
3413.707361	620213.412255	46.320359
3411.699592	611466.323404	46.325364
3409.668019	602622.923005	46.330369
3407.574894	593723.778801	46.335373
3405.633702	584753.187397	46.340378
3403.473025	575707.375130	46.345383
3401.544249	566595.569695	46.350388
3399.605143	557414.399290	46.355393
3397.448195	548165.374217	46.360397
3395.398031	538842.511767	46.365402
3393.208985	529465.005185	46.370407
3390.721091	520019.153529	46.375412
3388.601371	510493.973274	46.380417
3386.692752	500929.375805	46.385421
3384.020802	491290.410802	46.390426
3381.964418	481579.236085	46.395431
3379.337577	471820.279015	46.400436
3377.128717	461992.254101	46.405441
3374.485739	452109.588297	46.410445
3372.265074	442169.517721	46.415450
3369.966004	432165.545469	46.420455
3367.108349	422104.546302	46.425460
3364.387449	411969.093262	46.430465
3361.799211	401797.978358	46.435469
3358.930547	391571.467125	46.440474
3356.320332	381305.544463	46.445479
3353.388322	370993.824048	46.450484
3350.623607	360617.455607	46.455489
3347.851101	350216.103938	46.460493
3344.565511	339759.649927	46.465498
3341.671985	329273.541951	46.470503
3338.288209	318736.960349	46.475508
3335.392277	308157.899255	46.480513
3332.294192	297549.528107	46.485517
3328.684481	286913.784932	46.490522
3325.640729	276231.857372	46.495527
3322.316967	265528.038905	46.500532
3318.796373	254800.525364	46.505537
3315.208390	244029.350524	46.510541
3311.502191	233244.143311	46.515546
3307.936840	222351.005065	46.520551
3304.469905	211528.232825	46.525556
3300.593624	200695.547961	46.530561
3296.525110	189838.111629	46.535565
3291.816407	178983.095600	46.540570
3287.818736	168120.299081	46.545575
3283.138929	157268.051887	46.550580
3278.729778	146399.220340	46.555585
3273.705945	135576.840357	46.560589
3268.707889	124752.033678	46.565594
3263.639097	113950.878720	46.570599
3258.208065	103186.273884	46.575604
3252.590105	92467.138848	46.580609
3246.512539	81778.910024	46.585613
3239.267704	71155.542072	46.590618
3231.836115	60620.266972	46.595623
3222.285619	50210.001715	46.600628
3204.119263	40165.659829	46.605633
3174.447920	30619.748194	46.610637
3143.769473	21469.570104	46.615642
3104.003529	13072.475690	46.620647
3051.491431	5711.194889	46.625652
2944.842857	709.595622	46.630657
2721.489169	424.455754	46.635661
2592.910220	431.136141	46.640666
2576.390221	400.601495	46.645671
2634.564976	378.659411	46.650676
2720.816642	354.324179	46.655681
2796.000543	366.760538	46.660685
2844.197240	374.092049	46.665690
2863.543937	371.488423	46.670695
2862.009697	370.128526	46.675700
2850.955706	351.834921	46.680705
2837.975846	349.538956	46.685709
2826.509069	350.839763	46.690714
2819.908298	362.270713	46.695719
2816.499423	363.791129	46.700724
2816.055501	364.039773	46.705729
2815.462639	351.118865	46.710733
2814.069804	341.156125	46.715738
2812.640364	343.645291	46.720743
2809.606465	350.508106	46.725748
2805.963194	351.888894	46.730753
2802.922292	344.032619	46.735757
2800.362779	344.111407	46.740762
2797.742413	341.304997	46.745767
2794.412101	337.705906	46.750772
2790.989480	336.386938	46.755777
2787.980065	346.118557	46.760781
2785.147049	338.003177	46.765786
2782.187184	321.173013	46.770791
2778.937803	327.661725	46.775796
2775.633911	323.971274	46.780801
2772.129314	327.405181	46.785805
2768.201166	328.088279	46.790810
2765.178139	317.266478	46.795815
2762.008070	327.546088	46.800820
2759.694775	318.821562	46.805825
2756.198266	318.557711	46.810829
2752.426991	324.540330	46.815834
2749.576839	313.645148	46.820839
2746.186322	316.833735	46.825844
2742.536187	302.683424	46.830849
2739.240509	305.838914	46.835853
2736.035851	309.122749	46.840858
2732.749910	306.782657	46.845863
2728.967079	311.983841	46.850868
2725.565392	309.278168	46.855873
2722.776379	296.099057	46.860877
2719.433427	312.162593	46.865882
2715.923074	298.933612	46.870887
2712.368592	312.907129	46.875892
2708.956497	306.782010	46.880897
2705.489090	297.741098	46.885901
2702.115114	300.576835	46.890906
2699.202637	295.354549	46.895911
2695.455767	298.348062	46.900916
2691.787837	294.455645	46.905921
2688.196864	296.734034	46.910925
2684.888819	299.435980	46.915930
2681.547201	290.138552	46.920935
2677.992209	293.355762	46.925940
2674.944944	287.835469	46.930945
2671.790777	293.637731	46.935949
2667.822371	294.185449	46.940954
2664.687890	288.509454	46.945959
2661.197479	293.314283	46.950964
2657.873715	291.662487	46.955969
2654.514355	287.576750	46.960973
2650.836929	291.963623	46.965978
2647.487634	294.714906	46.970983
2643.409174	288.227920	46.975988
2640.717373	287.415692	46.980993
2637.512471	288.052509	46.985997
2633.877211	282.574829	46.991002
2630.287579	280.576694	46.996007
2626.829494	292.342837	47.001012
2623.341811	292.762968	47.006017
2619.819027	274.449114	47.011021
2616.448648	284.424655	47.016026
2612.914931	278.732929	47.021031
2608.606218	273.202837	47.026036
2605.736261	285.189584	47.031041
2602.403231	287.120624	47.036045
2599.238549	272.555440	47.041050
2596.024079	271.391965	47.046055
2591.657231	278.951230	47.051060
2588.063349	269.272121	47.056065
2584.778706	274.171695	47.061069
2581.431097	281.233875	47.066074
2578.712121	267.541835	47.071079
2575.045231	282.825235	47.076084
2571.805675	274.722861	47.081089
2567.745047	267.834807	47.086093
2564.116324	274.984091	47.091098
2561.536170	262.449614	47.096103
2557.538812	262.344213	47.101108
2554.024143	271.930481	47.106113
2550.905655	259.533223	47.111117
2546.872703	263.596658	47.116122
2543.417635	267.404879	47.121127
2540.343689	262.364686	47.126132
2536.568939	261.660339	47.131137
2533.317854	262.942241	47.136141
2529.837197	263.175780	47.141146
2526.249698	256.540536	47.146151
2522.504975	262.237284	47.151156
2518.996369	267.344391	47.156161
2515.307878	255.818770	47.161165
2511.683148	253.975162	47.166170
2509.003611	253.451015	47.171175
2505.378819	256.096736	47.176180
2502.166614	249.934838	47.181185
2498.793580	253.225801	47.186189
2494.901609	257.211947	47.191194
2491.658202	252.480110	47.196199
2487.912062	258.924042	47.201204
2484.558718	252.134483	47.206209
2480.957665	258.419232	47.211213
2476.776091	249.962009	47.216218
2474.054984	242.990456	47.221223
2470.358279	252.044118	47.226228
2467.061197	249.861084	47.231233
2463.839884	248.273484	47.236237
2460.179412	253.375368	47.241242
2456.704778	248.946872	47.246247
2452.638634	247.261920	47.251252
2449.366963	235.080013	47.256257
2446.221053	249.180041	47.261261
2442.620897	244.109966	47.266266
2439.268073	244.716899	47.271271
2435.220265	253.897734	47.276276
2432.184865	233.541773	47.281281
2428.780443	247.469955	47.286285
2425.274318	246.097258	47.291290
2421.807218	236.006774	47.296295
2418.095328	246.197911	47.301300
2414.949125	250.672781	47.306305
2410.709923	241.253531	47.311309
2407.716895	250.781237	47.316314
2404.722530	237.700135	47.321319
2400.584715	241.155640	47.326324
2396.933191	237.063964	47.331329
2393.474473	246.571198	47.336333
2389.911475	249.580986	47.341338
2387.066309	237.911938	47.346343
2383.505465	241.567381	47.351348
2379.860543	241.985241	47.356353
2376.717396	244.736074	47.361357
2372.603640	251.626727	47.366362
2369.283952	228.854516	47.371367
2365.811854	243.689486	47.376372
2362.411670	246.281554	47.381377
2358.796980	245.648571	47.386381
2354.913168	250.461172	47.391386
2351.922935	234.983228	47.396391
2348.582777	242.322658	47.401396
2344.696610	242.031907	47.406401
2341.220356	233.804744	47.411405
2337.952221	239.279810	47.416410
2334.885836	234.403035	47.421415
2331.556953	240.096980	47.426420
2327.465532	245.002731	47.431425
2323.874887	234.622698	47.436429
2319.858762	238.165907	47.441434
2317.010846	235.347406	47.446439
2313.074220	234.768430	47.451444
2310.049670	237.561883	47.456449
2306.929084	230.564050	47.461453
2302.765312	237.168289	47.466458
2299.394146	232.897141	47.471463
2295.997208	236.434527	47.476468
2292.491831	227.308596	47.481473
2288.909051	228.693154	47.486477
2285.221614	237.931814	47.491482
2282.260174	225.846334	47.496487
2278.774277	226.450818	47.501492
2275.061559	228.800075	47.506497
2271.520398	223.081070	47.511501
2267.631460	228.347781	47.516506
2264.485182	232.934493	47.521511
2260.825446	226.667573	47.526516
2257.411681	225.430474	47.531521
2254.339804	229.085728	47.536525
2250.599054	231.660218	47.541530
2247.383264	222.611747	47.546535
2243.867923	228.987810	47.551540
2239.968764	224.629059	47.556545
2236.545954	225.612161	47.561549
2232.874469	225.267217	47.566554
2229.294668	219.735251	47.571559
2225.995862	226.391801	47.576564
2222.411597	221.267239	47.581569
2219.160418	225.866039	47.586573
2215.312799	227.387447	47.591578
2211.833979	221.905130	47.596583
2208.514352	219.545594	47.601588
2204.870591	227.147064	47.606593
2201.764511	234.082114	47.611597
2197.994316	234.467943	47.616602
2194.596188	220.415300	47.621607
2191.139853	230.565941	47.626612
2187.841409	223.045325	47.631617
2184.184296	228.667379	47.636621
2180.581564	227.410184	47.641626
2177.235613	219.818978	47.646631
2173.311364	225.481548	47.651636
2169.930303	222.093502	47.656641
2166.761381	219.175195	47.661645
2162.831017	222.744093	47.666650
2159.545940	220.888543	47.671655
2155.906041	222.301823	47.676660
2152.368221	225.857475	47.681665
2149.299544	216.675678	47.686669
2145.878893	231.298491	47.691674
2142.326295	217.489494	47.696679
2138.384730	222.832032	47.701684
2134.662311	228.359317	47.706689
2131.650233	218.150348	47.711693
2128.162533	227.513474	47.716698
2124.732210	219.641822	47.721703
2121.289597	225.716576	47.726708
2117.725294	219.272496	47.731713
2114.201328	221.010097	47.736717
2110.481040	225.777185	47.741722
2106.946306	217.751201	47.746727
2103.705929	226.129687	47.751732
2100.216968	222.584556	47.756737
2097.130322	211.682611	47.761741
2093.013307	223.852265	47.766746
2089.474469	218.867576	47.771751
2085.773173	219.260447	47.776756
2082.450009	221.128117	47.781761
2078.937394	216.583558	47.786765
2075.240553	219.358659	47.791770
2072.194507	220.632580	47.796775
2068.808206	216.762721	47.801780
2064.938686	214.757577	47.806785
2061.836249	217.875132	47.811789
2058.549688	218.619188	47.816794
2054.724776	213.833841	47.821799
2051.303958	218.475487	47.826804
2047.571117	217.079900	47.831809
2044.014938	213.645433	47.836813
2040.172206	226.530016	47.841818
2037.062310	209.113283	47.846823
2033.630718	210.117756	47.851828
2030.226641	218.682896	47.856833
2026.843191	211.895503	47.861837
2022.894931	216.973319	47.866842
2019.356560	213.868992	47.871847
2015.826015	207.094134	47.876852
2012.441647	214.262105	47.881857
2009.243405	209.183390	47.886861
2005.611449	206.970781	47.891866
2002.078071	206.622210	47.896871
1998.723206	197.718474	47.901876
1995.289534	207.959650	47.906881
1991.847369	200.166395	47.911885
1988.323050	202.736280	47.916890
1984.834592	201.549618	47.921895
1981.100236	205.807052	47.926900
1977.464374	215.519153	47.931905
1973.896752	217.355475	47.936909
1970.338013	215.818541	47.941914
1967.208082	213.970635	47.946919
1963.612658	198.505580	47.951924
1960.214736	202.355808	47.956929
1956.476935	202.077981	47.961933
1953.043474	205.343715	47.966938
1949.459497	197.278503	47.971943
1945.829020	203.165099	47.976948
1942.542175	207.471450	47.981953
1939.438484	205.487128	47.986957
1935.364892	207.833139	47.991962
1932.499441	202.595972	47.996967
1928.616500	202.850877	48.001972
1925.279776	202.193366	48.006977
1922.017570	205.070269	48.011981
1918.232608	206.215670	48.016986
1914.621396	208.684990	48.021991
1911.200539	210.350622	48.026996
1907.668058	201.899870	48.032001
1904.166682	203.218989	48.037005
1900.235144	205.983958	48.042010
1896.942929	200.102943	48.047015
1893.350604	211.586868	48.052020
1889.957584	209.154849	48.057025
1886.525911	192.758744	48.062029
1882.853647	207.625770	48.067034
1880.014446	212.278767	48.072039
1876.376104	207.023228	48.077044
1872.912842	209.673068	48.082049
1869.065178	195.936329	48.087053
1865.155009	208.872048	48.092058
1861.698437	204.328918	48.097063
1858.529343	207.663347	48.102068
1854.905737	208.205609	48.107073
1851.909720	196.266772	48.112077
1848.147899	203.335776	48.117082
1844.741204	198.270328	48.122087
1841.102715	198.292370	48.127092
1837.554081	209.528285	48.132097
1834.314580	192.304152	48.137101
1830.422987	211.097907	48.142106
1826.983462	198.784259	48.147111
1823.333266	196.482118	48.152116
1819.996575	197.610037	48.157121
1817.033168	197.456086	48.162125
1813.241155	195.983571	48.167130
1809.726973	199.818811	48.172135
1806.145175	195.296475	48.177140
1802.398247	193.449723	48.182145
1799.115290	197.256089	48.187149
1795.510710	195.471388	48.192154
1792.126754	193.321168	48.197159
1788.292768	199.491110	48.202164
1784.486792	193.338481	48.207169
1781.812211	192.195606	48.212173
1777.875241	201.725225	48.217178
1774.377489	198.931902	48.222183
1771.247880	200.538196	48.227188
1767.635087	197.392023	48.232193
1764.397481	192.183095	48.237197
1760.500090	189.922369	48.242202
1757.074130	196.791559	48.247207
1753.299476	198.773233	48.252212
1749.975314	190.833874	48.257217
1746.706294	180.608138	48.262221
1743.476969	199.065622	48.267226
1739.253255	198.306239	48.272231
1736.034061	196.637137	48.277236
1732.223691	197.565835	48.282241
1729.040029	192.793260	48.287245
1725.396996	193.493782	48.292250
1722.171070	195.663531	48.297255
1718.392363	187.621121	48.302260
1714.882187	201.916378	48.307265
1711.634903	195.697746	48.312269
1708.101937	199.262656	48.317274
1704.765387	194.013357	48.322279
1701.240624	192.633147	48.327284
1697.465809	200.331224	48.332289
1694.306172	197.800514	48.337293
1690.535139	195.769563	48.342298
1687.232961	184.310601	48.347303
1683.299755	196.563340	48.352308
1679.711220	191.204693	48.357313
1676.356515	182.064839	48.362317
1672.431498	197.817643	48.367322
1669.244418	183.885325	48.372327
1665.974136	186.731209	48.377332
1662.758949	192.827804	48.382337
1659.375562	189.717729	48.387341
1655.405858	201.578429	48.392346
1651.972041	187.281851	48.397351
1648.469243	189.117099	48.402356
1644.926751	193.068172	48.407361
1641.538287	187.863485	48.412365
1637.773479	189.585803	48.417370
1634.512495	190.511597	48.422375
1631.090247	183.969583	48.427380
1627.319301	189.630191	48.432385
1624.047724	193.780839	48.437389
1620.431180	190.758687	48.442394
1616.972481	186.424604	48.447399
1613.361123	190.377880	48.452404
1610.012050	186.372092	48.457409
1606.303448	182.220335	48.462413
1602.590317	193.412737	48.467418
1599.528746	190.249486	48.472423
1595.938762	187.726605	48.477428
1592.408130	177.591586	48.482433
1588.846189	181.164783	48.487437
1585.433287	192.952264	48.492442
1582.152175	174.156681	48.497447
1578.732322	189.792504	48.502452
1574.785467	187.146902	48.507457
1571.623214	181.939651	48.512461
1567.652303	186.480390	48.517466
1564.308785	174.988868	48.522471
1561.160164	185.932341	48.527476
1557.133402	186.458119	48.532481
1554.083139	175.929333	48.537485
1550.305429	182.357156	48.542490
1546.800727	178.060993	48.547495
1543.499458	185.543750	48.552500
1539.706768	186.459470	48.557505
1536.617071	180.326311	48.562509
1532.915734	185.836863	48.567514
1529.474736	183.850981	48.572519
1525.865675	182.880682	48.577524
1521.909556	185.590018	48.582529
1518.697402	182.366322	48.587533
1515.391477	179.376034	48.592538
1512.145121	172.279522	48.597543
1508.324844	178.821529	48.602548
1504.512702	183.476584	48.607553
1501.339430	172.875886	48.612557
1497.796653	185.440829	48.617562
1494.363214	185.385799	48.622567
1490.998685	178.715557	48.627572
1487.504826	183.626292	48.632577
1483.842621	176.500559	48.637581
1480.151775	183.985582	48.642586
1476.931325	187.400263	48.647591
1473.616217	179.245782	48.652596
1469.694149	178.955513	48.657601
1466.775714	174.185374	48.662605
1462.810600	182.925095	48.667610
1459.190128	172.481002	48.672615
1455.519555	181.923083	48.677620
1451.901572	182.516316	48.682625
1448.978269	184.348259	48.687629
1445.257120	183.214283	48.692634
1442.158883	175.418356	48.697639
1438.698062	181.055193	48.702644
1434.916109	180.865927	48.707649
1431.492048	178.640625	48.712653
1427.237207	180.025136	48.717658
1424.327279	173.999005	48.722663
1420.615259	173.259247	48.727668
1417.227008	184.064146	48.732673
1413.907665	175.485192	48.737677
1410.231663	182.135140	48.742682
1406.521849	177.080701	48.747687
1403.219070	177.905174	48.752692
1399.674071	188.056313	48.757697
1396.508336	169.510950	48.762701
1392.734138	178.205773	48.767706
1389.254412	175.489594	48.772711
1385.739988	171.955171	48.777716
1381.782054	181.685631	48.782721
1378.884144	171.733401	48.787725
1375.064610	183.538643	48.792730
1371.796492	166.430548	48.797735
1368.286271	165.339444	48.802740
1365.047458	167.048383	48.807745
1361.725518	163.337476	48.812749
1357.445340	178.333813	48.817754
1354.160705	181.178648	48.822759
1350.892154	171.624817	48.827764
1347.339854	178.243225	48.832769
1344.016816	164.566590	48.837773
1340.152378	174.326027	48.842778
1336.630819	174.032272	48.847783
1333.175542	174.007761	48.852788
1329.888159	174.679968	48.857793
1326.445047	160.527027	48.862797
1322.585482	172.815299	48.867802
1318.925496	173.073592	48.872807
1315.836474	169.462182	48.877812
1311.844935	179.926892	48.882817
1308.963007	166.068154	48.887821
1305.530897	169.594400	48.892826
1301.930607	172.775293	48.897831
1297.983594	169.789918	48.902836
1294.093120	172.984680	48.907841
1290.754746	171.074917	48.912845
1287.640172	174.784347	48.917850
1284.397214	171.484068	48.922855
1280.707848	169.609460	48.927860
1277.385918	168.684238	48.932865
1274.072745	170.443574	48.937869
1269.941770	169.677754	48.942874
1266.847931	162.161975	48.947879
1263.256548	176.206275	48.952884
1259.570533	167.818760	48.957889
1255.935393	166.911709	48.962893
1252.956397	172.201336	48.967898
1249.159552	171.137482	48.972903
1245.785962	167.339859	48.977908
1242.043993	174.163059	48.982913
1238.622356	173.254808	48.987917
1235.314006	167.985921	48.992922
1231.264775	169.077440	48.997927
1227.974590	166.596825	49.002932
1224.647648	166.292310	49.007937
1221.224402	168.727677	49.012941
1217.539518	164.765501	49.017946
1214.374854	169.752730	49.022951
1210.724234	169.219401	49.027956
1206.901777	175.078425	49.032961
1203.539022	159.127519	49.037965
1200.124441	161.359320	49.042970
1196.810558	173.358082	49.047975
1193.230842	167.820094	49.052980
1189.189218	170.336350	49.057985
1185.754547	169.781788	49.062989
1182.494603	164.431836	49.067994
1179.084401	163.210471	49.072999
1175.239110	177.007660	49.078004
1172.198344	166.231674	49.083009
1169.030215	168.507055	49.088013
1164.805970	173.848684	49.093018
1161.438967	160.226879	49.098023
1158.126184	156.113238	49.103028
1154.369459	176.156595	49.108033
1151.012028	166.513079	49.113037
1147.472508	163.413762	49.118042
1144.156518	158.437223	49.123047
1140.812848	164.036791	49.128052
1137.157131	178.007311	49.133057
1134.122918	167.940486	49.138061
1130.173579	162.575434	49.143066
1126.427129	167.616523	49.148071
1123.230938	171.568869	49.153076
1119.235014	181.969282	49.158081
1115.874270	165.960086	49.163085
1112.562209	167.182824	49.168090
1108.969065	179.643067	49.173095
1105.418544	161.497257	49.178100
1101.634932	175.610940	49.183105
1098.742218	166.826383	49.188109
1094.893606	170.815323	49.193114
1091.518755	170.605403	49.198119
1088.120170	161.411292	49.203124
1084.589324	176.175715	49.208129
1081.294228	167.211453	49.213133
1077.422894	169.444041	49.218138
1073.613275	167.647313	49.223143
1070.482649	168.667765	49.228148
1066.769353	164.376616	49.233153
1063.727195	166.155332	49.238157
1059.753446	168.618625	49.243162
1056.521228	171.308928	49.248167
1053.231554	167.220528	49.253172
1049.475667	167.298080	49.258177
1046.198510	168.967028	49.263181
1042.370200	160.640341	49.268186
1038.615104	168.228310	49.273191
1035.698570	157.367968	49.278196
1031.888393	167.017363	49.283201
1028.618158	160.216493	49.288205
1024.877211	163.449454	49.293210
1021.479453	164.743506	49.298215
1018.055680	162.620583	49.303220
1014.242475	167.058224	49.308225
1010.835058	154.112868	49.313229
1007.011912	175.938204	49.318234
1003.900362	161.246331	49.323239
1000.546891	155.373955	49.328244
996.804328	163.236995	49.333249
993.749795	155.755818	49.338253
989.849667	162.624486	49.343258
986.260831	166.356212	49.348263
983.092495	159.322389	49.353268
979.103188	163.654065	49.358273
976.025136	166.067279	49.363277
972.625233	167.607953	49.368282
968.675237	166.905272	49.373287
965.303664	160.295888	49.378292
961.801000	160.719492	49.383297
958.114268	168.489971	49.388301
954.805311	165.199971	49.393306
951.481756	165.799011	49.398311
948.242330	158.526756	49.403316
944.341023	162.588995	49.408321
940.699511	158.485355	49.413325
937.398803	158.861417	49.418330
934.120510	169.244241	49.423335
930.323720	161.828339	49.428340
926.770827	160.737805	49.433345
923.521117	165.955942	49.438349
919.955829	166.014623	49.443354
916.627765	160.134545	49.448359
912.750954	158.507448	49.453364
909.012876	163.826852	49.458369
905.695462	155.701503	49.463373
902.110936	164.883954	49.468378
898.984165	168.904843	49.473383
895.621436	154.042709	49.478388
891.378019	166.527634	49.483393
888.135697	160.814940	49.488397
884.663511	157.543350	49.493402
881.314741	172.395078	49.498407
878.157363	159.883737	49.503412
874.258771	173.820964	49.508417
870.958628	158.510871	49.513421
867.283169	163.312571	49.518426
863.675101	162.513238	49.523431
860.657289	152.202261	49.528436
856.542260	162.119315	49.533441
853.525167	165.040554	49.538445
849.580255	171.107323	49.543450
846.321681	158.413232	49.548455
842.991568	158.625102	49.553460
839.237920	158.287754	49.558465
835.644095	157.017966	49.563469
831.832627	154.573819	49.568474
828.589957	158.677015	49.573479
825.440946	160.300832	49.578484
821.892679	160.779196	49.583489
818.472854	156.118909	49.588493
814.663661	155.449795	49.593498
811.028145	157.237225	49.598503
807.999224	157.579419	49.603508
804.304103	155.775092	49.608513
800.804615	157.508888	49.613517
797.224746	158.924973	49.618522
794.165302	159.944549	49.623527
790.558310	166.207705	49.628532
786.602850	157.953586	49.633537
782.958551	155.783056	49.638541
779.283831	159.031647	49.643546
775.881124	159.236794	49.648551
772.804886	159.127381	49.653556
769.249477	159.993286	49.658561
765.721956	156.928113	49.663565
762.266087	159.082691	49.668570
758.870591	156.889731	49.673575
755.285050	161.610933	49.678580
751.686702	159.999703	49.683585
748.266894	151.121751	49.688589
744.493840	168.801101	49.693594
740.846357	156.081038	49.698599
737.557457	154.830399	49.703604
734.078225	157.744943	49.708609
731.189785	150.801083	49.713613
727.585592	152.854685	49.718618
723.550449	154.153423	49.723623
720.069209	150.096845	49.728628
716.488279	160.269180	49.733633
713.006773	161.164048	49.738637
709.484923	154.751195	49.743642
706.211094	159.805398	49.748647
703.078859	148.160751	49.753652
699.257320	162.926058	49.758657
695.721076	153.703625	49.763661
692.100467	161.511745	49.768666
688.534072	157.586449	49.773671
685.242094	141.141405	49.778676
681.244785	161.701243	49.783681
678.163040	155.278071	49.788685
674.749257	150.362931	49.793690
671.003613	161.639408	49.798695
667.886134	147.690033	49.803700
664.023890	156.607985	49.808705
660.572018	151.893297	49.813709
656.757349	148.987193	49.818714
653.438127	160.447580	49.823719
650.238650	159.695222	49.828724
646.664894	154.097880	49.833729
643.009164	153.597870	49.838733
639.736989	152.412197	49.843738
636.301370	155.727228	49.848743
632.977484	153.502975	49.853748
628.799425	159.979013	49.858753
625.385950	140.656383	49.863757
622.075973	150.241200	49.868762
618.836351	145.408217	49.873767
615.225534	149.933192	49.878772
611.485164	150.015038	49.883777
607.653175	150.753474	49.888781
604.454864	154.156687	49.893786
600.706875	145.118757	49.898791
597.486182	157.443187	49.903796
593.981965	153.026636	49.908801
590.940850	148.493247	49.913805
587.603943	162.496354	49.918810
583.715272	156.879441	49.923815
580.075435	152.423641	49.928820
576.230578	159.589615	49.933825
573.004897	147.115503	49.938829
569.584965	153.831765	49.943834
565.962426	152.161104	49.948839
562.360704	149.214753	49.953844
558.732434	153.890032	49.958849
555.417362	138.948645	49.963853
551.879986	143.879816	49.968858
548.484453	148.093918	49.973863
545.118378	156.685111	49.978868
541.197159	160.932089	49.983873
537.791094	146.140993	49.988877
534.576900	148.292465	49.993882
530.954701	157.634116	49.998887
527.367495	154.796965	50.003892
523.613301	157.035767	50.008897
520.625923	149.429121	50.013901
517.361329	154.188185	50.018906
513.511116	149.601535	50.023911
510.397377	153.984670	50.028916
506.323360	158.616405	50.033921
502.631328	152.169441	50.038925
499.215515	153.937812	50.043930
495.712766	161.521649	50.048935
492.444171	152.853082	50.053940
488.887389	149.369673	50.058945
485.903183	153.894597	50.063949
482.040445	152.349590	50.068954
478.117150	158.051117	50.073959
474.960384	151.804710	50.078964
471.308403	145.957584	50.083969
468.066193	149.944057	50.088973
464.178479	149.657287	50.093978
460.672867	136.682259	50.098983
457.729906	139.714637	50.103988
453.859608	147.691571	50.108993
450.324267	144.016411	50.113997
447.218670	152.683888	50.119002
443.238496	143.508026	50.124007
440.216278	144.472977	50.129012
436.324766	143.674932	50.134017
432.487639	147.469753	50.139021
429.379783	156.038760	50.144026
425.902990	141.332532	50.149031
422.444909	141.487226	50.154036
418.878626	157.302290	50.159041
415.743639	153.025610	50.164045
411.791184	152.783406	50.169050
408.091687	153.650124	50.174055
405.018423	152.290832	50.179060
401.142406	155.814680	50.184065
397.721100	143.137905	50.189069
394.272648	147.502887	50.194074
390.627659	141.814281	50.199079
387.387388	141.145549	50.204084
383.888964	149.440708	50.209089
380.604610	143.821570	50.214093
377.381322	145.100045	50.219098
373.167659	145.134533	50.224103
369.951994	138.598702	50.229108
366.020819	151.433923	50.234113
362.894863	146.942096	50.239117
359.446549	143.019886	50.244122
355.900633	139.230512	50.249127
352.669270	133.901562	50.254132
348.607205	142.061368	50.259137
344.835883	141.360824	50.264141
341.753482	143.538658	50.269146
337.978438	148.063973	50.274151
334.688098	140.506696	50.279156
330.966798	147.442344	50.284161
328.047926	135.257178	50.289165
324.545833	144.045945	50.294170
321.135558	145.791295	50.299175
317.560109	137.496238	50.304180
313.784409	141.415737	50.309185
310.046544	144.826737	50.314189
306.586807	146.042007	50.319194
303.094932	139.527875	50.324199
299.915437	145.987296	50.329204
296.314578	136.348239	50.334209
292.782539	134.639701	50.339213
289.195516	147.176491	50.344218
285.612335	144.078174	50.349223
282.255863	139.126569	50.354228
278.314343	156.569527	50.359233
275.253316	136.651459	50.364237
271.993804	146.646571	50.369242
268.305399	145.657619	50.374247
264.824002	132.612433	50.379252
261.221610	140.179289	50.384257
257.757311	138.747946	50.389261
254.097837	149.138952	50.394266
250.484456	138.316955	50.399271
247.473335	136.867763	50.404276
244.078054	149.104750	50.409281
240.112415	140.865431	50.414285
236.547145	137.151937	50.419290
232.737338	150.781758	50.424295
229.518673	142.366047	50.429300
226.182137	144.245073	50.434305
222.740808	134.691680	50.439309
219.430768	133.118952	50.444314
215.827991	148.151669	50.449319
212.119862	133.902118	50.454324
208.297761	146.012924	50.459329
205.157171	136.991319	50.464333
201.885586	129.842220	50.469338
197.918675	143.252853	50.474343
194.972698	144.362574	50.479348
191.085129	145.822328	50.484353
187.587257	134.513767	50.489357
184.021650	136.809005	50.494362
180.725411	142.822709	50.499367
177.616535	127.001065	50.504372
173.503328	141.780639	50.509377
170.038976	134.473893	50.514381
166.661973	139.896000	50.519386
162.853451	141.447382	50.524391
159.922507	139.894123	50.529396
156.127680	142.202885	50.534401
152.776605	133.236416	50.539405
149.357259	135.972461	50.544410
145.323100	135.522149	50.549415
142.248264	138.379145	50.554420
138.850161	144.604247	50.559425
135.180531	133.907842	50.564429
131.223598	136.139225	50.569434
127.296648	135.952374	50.574439
124.701289	137.008135	50.579444
121.105846	142.982422	50.584449
117.536230	131.855057	50.589453
114.326503	132.698722	50.594458
110.934233	135.087390	50.599463
106.857747	130.562770	50.604468
103.339413	139.437780	50.609473
100.206854	133.010310	50.614477
96.749470	134.354934	50.619482
92.810766	134.306190	50.624487
89.635416	138.146631	50.629492
85.946533	136.796201	50.634497
82.278900	132.957852	50.639501
79.092902	128.599917	50.644506
75.603103	145.002971	50.649511
72.159193	129.567843	50.654516
68.191040	136.618404	50.659521
64.737271	132.990472	50.664525
61.353023	136.230212	50.669530
58.181160	143.672256	50.674535
54.728359	139.683389	50.679540
51.165824	138.964993	50.684545
47.687315	136.407907	50.689549
44.322611	135.653567	50.694554
40.220236	143.670350	50.699559
36.786902	142.876055	50.704564
33.582356	146.007783	50.709569
30.133730	139.488350	50.714573
26.704598	147.665379	50.719578
22.882539	143.602595	50.724583
19.622637	141.955096	50.729588
15.971954	140.499345	50.734593
12.179062	140.729521	50.739597
8.793292	141.624234	50.744602
5.135021	151.378248	50.749607
2.209076	133.890201	50.754612