Thu Jun 16 11:04:21 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.042095	106.986629	0.000000
0.687433	113.735903	0.005005
0.688705	110.837471	0.010010
1.184858	116.133649	0.015014
0.660165	99.208286	0.020019
1.024005	96.923452	0.025024
0.581250	78.827358	0.030029
0.423773	62.029584	0.035034
-0.150789	50.942562	0.040038
-0.459637	52.726691	0.045043
-0.449315	36.597315	0.050048
-1.040217	18.928776	0.055053
-1.351781	21.951354	0.060058
-1.460687	4.326298	0.065062
-2.010165	8.495969	0.070067
-2.110778	-1.224754	0.075072
-2.440383	-11.642794	0.080077
-3.131150	-9.118400	0.085082
-3.102011	-18.577814	0.090086
-3.551179	-13.187613	0.095091
-3.415981	-12.713196	0.100096
-3.685626	-15.629576	0.105101
-4.779344	-9.114755	0.110106
-4.954594	-17.685759	0.115110
-5.404280	-16.300205	0.120115
-5.385799	-2.735325	0.125120
-5.269523	-10.694716	0.130125
-5.547454	-17.521232	0.135130
-4.997770	-16.124241	0.140134
-5.277622	-14.125210	0.145139
-5.971362	-13.635050	0.150144
-6.963360	-6.107393	0.155149
-6.994356	-11.124673	0.160154
-6.778804	-4.635815	0.165158
-7.209649	-14.998745	0.170163
-7.793685	-12.490806	0.175168
-8.560402	-13.510017	0.180173
-8.534185	-11.028148	0.185178
-8.214183	-10.244213	0.190182
-8.429340	-17.191003	0.195187
-8.762866	-12.853601	0.200192
-8.608713	-12.642367	0.205197
-8.540026	-13.103538	0.210202
-9.145176	-14.255501	0.215206
-9.896949	-9.285966	0.220211
-9.678517	-15.321231	0.225216
-9.753633	-16.812747	0.230221
-10.920582	-10.418809	0.235226
-10.598429	-16.899074	0.240230
-11.452721	-9.298678	0.245235
-11.173130	-18.133373	0.250240
-11.275851	-16.335765	0.255245
-11.977849	-20.406264	0.260250
-12.759191	-25.142778	0.265254
-12.550321	-13.818219	0.270259
-12.449595	-19.969777	0.275264
-12.537232	-11.763973	0.280269
-12.840213	-4.922961	0.285274
-13.004367	-16.220999	0.290278
-13.441034	-14.862061	0.295283
-14.037399	-17.146240	0.300288
-14.617562	-16.631541	0.305293
-14.637252	-18.310779	0.310298
-14.396168	-20.299180	0.315302
-14.738654	-22.196862	0.320307
-14.684695	-28.169032	0.325312
-14.991944	-23.171349	0.330317
-16.031144	-22.396308	0.335322
-15.805680	-21.509344	0.340326
-16.154143	-1.873769	0.345331
-16.383470	-13.717739	0.350336
-16.396118	-15.672890	0.355341
-16.232574	-15.948879	0.360346
-16.584779	-21.823445	0.365350
-17.653709	-18.682421	0.370355
-17.964049	-20.346873	0.375360
-17.788831	-8.890868	0.380365
-17.947574	-11.590583	0.385370
-18.013218	-33.824227	0.390374
-18.772996	-18.104314	0.395379
-19.130075	-23.622034	0.400384
-19.036020	-16.953286	0.405389
-19.536500	-3.310242	0.410394
-19.257590	-22.807275	0.415398
-19.539280	-10.951293	0.420403
-19.719280	-17.097697	0.425408
-20.610948	-26.669915	0.430413
-21.048261	-21.582765	0.435418
-20.913436	-18.647283	0.440422
-20.712060	-15.328876	0.445427
-20.984438	-20.137861	0.450432
-21.227590	-13.583857	0.455437
-21.965802	-7.973342	0.460442
-22.398764	-22.266361	0.465446
-22.838243	-12.131947	0.470451
-22.701374	-22.207690	0.475456
-22.840504	-10.964326	0.480461
-22.915521	-20.913208	0.485466
-22.960850	-19.078322	0.490470
-23.629411	-10.419192	0.495475
-24.324090	-10.952108	0.500480
-24.539421	-14.724105	0.505485
-24.792183	-13.269184	0.510490
-24.439832	-27.169216	0.515494
-24.694169	-22.208985	0.520499
-24.648041	-18.557617	0.525504
-24.479961	-16.924230	0.530509
-25.356195	-11.628301	0.535514
-25.697410	-10.621841	0.540518
-26.214972	-11.040584	0.545523
-26.401613	-16.227078	0.550528
-26.700230	-8.128467	0.555533
-26.964682	0.010968	0.560538
-27.455445	-6.788763	0.565542
-27.786857	-8.797387	0.570547
-27.845337	-17.254504	0.575552
-28.084429	-17.637583	0.580557
-28.375494	-16.339011	0.585562
-27.891188	-21.523624	0.590566
-28.345221	-10.102732	0.595571
-27.960127	-20.061159	0.600576
-28.822453	-9.269482	0.605581
-29.297622	-4.672987	0.610586
-29.341742	-8.825275	0.615590
-30.390593	-15.999698	0.620595
-30.849444	-9.260883	0.625600
-30.244928	-14.959716	0.630605
-30.412423	-11.575613	0.635610
-30.595702	-11.616611	0.640614
-31.120836	-5.975605	0.645619
-31.184326	-15.474956	0.650624
-31.593819	-13.965721	0.655629
-32.172633	-5.011747	0.660634
-32.251667	-20.217989	0.665638
-32.664744	-17.432181	0.670643
-32.502548	-8.015260	0.675648
-32.573279	-16.775487	0.680653
-32.573473	-18.250578	0.685658
-32.790814	-18.640900	0.690662
-33.895917	-17.618395	0.695667
-33.908623	-17.882422	0.700672
-33.858915	-25.096624	0.705677
-34.055002	-10.202557	0.710682
-34.151265	-21.526014	0.715686
-34.779099	-14.072253	0.720691
-35.218776	-18.939220	0.725696
-35.271108	-18.002402	0.730701
-35.256911	-12.022768	0.735706
-36.091734	-20.301664	0.740710
-36.863741	-13.112144	0.745715
-37.063413	-23.958389	0.750720
-36.314953	-22.353637	0.755725
-36.737225	-10.096581	0.760730
-36.890276	-30.186349	0.765734
-37.268479	-8.116042	0.770739
-37.033387	-18.981066	0.775744
-37.719211	-17.818015	0.780749
-38.872030	-10.797888	0.785754
-38.817370	-21.680840	0.790758
-39.177749	-10.941632	0.795763
-39.118478	-12.981475	0.800768
-38.639610	-6.936078	0.805773
-39.125985	-9.142739	0.810778
-39.065659	-22.054544	0.815782
-39.957643	-6.369595	0.820787
-40.230840	-9.250858	0.825792
-40.230540	-21.866649	0.830797
-40.742867	-0.413044	0.835802
-40.378297	-13.369414	0.840806
-41.309477	-10.713243	0.845811
-41.608313	-6.878587	0.850816
-41.853417	-12.351775	0.855821
-42.208285	-16.188512	0.860826
-41.875857	-9.547515	0.865830
-42.321579	-17.858160	0.870835
-42.428451	-26.370312	0.875840
-42.506258	-21.044444	0.880845
-43.546697	-12.222343	0.885850
-43.974957	-16.445708	0.890854
-44.099649	-10.426251	0.895859
-44.284262	-16.098651	0.900864
-43.852113	-13.790216	0.905869
-44.351093	-8.067211	0.910874
-43.980872	-14.889065	0.915878
-44.262153	-19.260924	0.920883
-44.894136	-22.250897	0.925888
-45.274248	-18.684467	0.930893
-45.593666	-11.474246	0.935898
-45.618169	-20.242504	0.940902
-46.598406	-22.350083	0.945907
-46.746557	-19.153365	0.950912
-46.958425	-27.488641	0.955917
-47.291310	-5.944639	0.960922
-47.072856	-19.756942	0.965926
-47.332534	-21.201678	0.970931
-47.480485	-17.667401	0.975936
-47.231352	-26.805841	0.980941
-47.845399	-9.152429	0.985946
-48.266782	-14.187367	0.990950
-48.678926	-8.440040	0.995955
-48.568270	-18.637037	1.000960
-49.052589	-22.156912	1.005965
-50.440687	-13.129573	1.010970
-49.525625	-10.485814	1.015974
-50.129795	-15.459665	1.020979
-50.238983	-14.379479	1.025984
-50.146785	-14.676529	1.030989
-50.579110	-10.639179	1.035994
-50.336463	-18.269327	1.040998
-51.256480	-11.980318	1.046003
-51.876334	-11.884448	1.051008
-51.813412	-20.901750	1.056013
-52.439591	-7.703977	1.061018
-52.041634	-18.208702	1.066022
-52.321165	-21.214698	1.071027
-52.147779	-14.073787	1.076032
-52.185230	-26.083226	1.081037
-53.030086	-9.922176	1.086042
-53.246118	-20.569595	1.091046
-53.806771	-12.963073	1.096051
-54.260884	-10.110796	1.101056
-53.737048	-19.826971	1.106061
-54.784825	-6.656104	1.111066
-55.084189	-12.857262	1.116070
-55.028924	-8.676551	1.121075
-55.429750	-8.862920	1.126080
-55.187670	-17.882703	1.131085
-55.556140	-6.343261	1.136090
-55.179025	-16.612806	1.141094
-56.187816	-20.614148	1.146099
-56.678114	-9.285917	1.151104
-56.639914	-16.338500	1.156109
-57.128496	-15.600783	1.161114
-57.289323	-5.974015	1.166118
-57.060296	-11.846379	1.171123
-57.746647	-15.197415	1.176128
-58.019701	-11.376394	1.181133
-58.487563	-12.612699	1.186138
-58.409238	-15.877117	1.191142
-58.500656	-15.495472	1.196147
-58.724498	-21.013504	1.201152
-58.443608	-18.503978	1.206157
-59.592901	-10.379417	1.211162
-59.783010	-19.047795	1.216166
-60.052138	-15.415062	1.221171
-60.070097	-13.792266	1.226176
-60.089592	-16.237282	1.231181
-60.678992	-10.121690	1.236186
-61.268006	-23.771142	1.241190
-61.433847	-6.220509	1.246195
-61.839094	-10.555208	1.251200
-61.648541	-9.616997	1.256205
-61.819112	-8.878958	1.261210
-61.621700	-10.979908	1.266214
-62.253781	-4.132257	1.271219
-63.143620	-2.864849	1.276224
-63.175842	-8.724917	1.281229
-63.791784	-3.620966	1.286234
-63.328663	-16.344420	1.291238
-63.308433	-10.558060	1.296243
-63.439603	-4.615073	1.301248
-63.682111	-17.968616	1.306253
-64.878694	-8.475514	1.311258
-65.000902	-7.156310	1.316262
-65.180735	-17.317333	1.321267
-65.472379	-17.602444	1.326272
-65.091979	-21.053911	1.331277
-65.298963	-17.890383	1.336282
-65.543872	-16.092460	1.341286
-66.457728	-20.291899	1.346291
-66.890690	-5.635407	1.351296
-66.735647	-18.681545	1.356301
-66.766601	-12.393559	1.361306
-66.739301	-18.279934	1.366310
-67.648677	-5.278438	1.371315
-68.270164	-19.243544	1.376320
-68.103823	-14.882209	1.381325
-68.323446	-7.269795	1.386330
-68.378254	-18.550971	1.391334
-68.553195	-8.623151	1.396339
-68.365098	0.180305	1.401344
-68.699797	-24.379020	1.406349
-69.584460	-14.599387	1.411354
-69.753058	-15.239761	1.416358
-69.786921	-16.052946	1.421363
-70.079607	-16.346763	1.426368
-70.193803	-15.011718	1.431373
-71.241884	-10.179564	1.436378
-71.438678	-9.658371	1.441382
-71.776070	-14.782262	1.446387
-71.608684	-12.647209	1.451392
-71.685632	-11.800339	1.456397
-71.682256	-19.483478	1.461402
-71.447400	-13.755577	1.466406
-71.966758	-17.795185	1.471411
-73.047738	-9.136359	1.476416
-73.195352	-14.071223	1.481421
-73.957672	-14.430669	1.486426
-73.239203	-26.295513	1.491430
-73.556315	-12.269429	1.496435
-73.381280	-17.250611	1.501440
-73.962200	-12.084774	1.506445
-74.766430	-9.041451	1.511450
-74.620914	-13.736988	1.516454
-75.000600	-17.110587	1.521459
-75.138897	-7.387313	1.526464
-74.701032	-21.212789	1.531469
-75.662345	-18.649499	1.536474
-76.194498	-19.906746	1.541478
-76.004560	-19.979532	1.546483
-76.534750	-13.980271	1.551488
-76.426208	-18.921755	1.556493
-76.978279	-14.293118	1.561498
-77.868182	-18.566952	1.566502
-78.211264	-25.599233	1.571507
-78.294869	-20.736374	1.576512
-77.640711	-29.814190	1.581517
-78.253021	-20.223605	1.586522
-78.363482	-18.466941	1.591526
-78.154827	-18.130449	1.596531
-78.477744	-15.114880	1.601536
-79.290398	-15.580148	1.606541
-80.125529	-12.672891	1.611546
-79.998023	-7.988459	1.616550
-79.865296	-14.733180	1.621555
-80.238398	-8.562770	1.626560
-80.115005	-11.394347	1.631565
-80.605989	-14.587661	1.636570
-81.052209	-14.313313	1.641574
-81.207054	-7.323749	1.646579
-81.646896	-6.480534	1.651584
-81.545993	-15.837266	1.656589
-81.552309	-16.188671	1.661594
-82.098701	-11.826447	1.666598
-82.487961	-16.012450	1.671603
-83.378413	-8.541032	1.676608
-83.353498	-8.578455	1.681613
-83.471567	-9.994997	1.686618
-83.202155	-12.533635	1.691622
-83.093008	-18.718841	1.696627
-83.439548	-19.217736	1.701632
-84.221408	-21.548199	1.706637
-84.630083	-13.892508	1.711642
-84.766398	-27.620320	1.716646
-84.308858	-20.143998	1.721651
-85.323615	-23.474985	1.726656
-85.653980	-22.900148	1.731661
-85.754746	-17.602450	1.736666
-86.017777	-18.351815	1.741670
-86.198441	-19.546598	1.746675
-86.237872	-15.435377	1.751680
-86.527375	-19.548782	1.756685
-87.453810	-12.508847	1.761690
-87.582521	-22.729415	1.766694
-87.896744	-9.204571	1.771699
-87.937012	-12.455209	1.776704
-87.734867	-20.814909	1.781709
-87.871017	-6.018454	1.786714
-87.788405	-15.797260	1.791718
-88.967746	-9.474661	1.796723
-89.165539	-13.801913	1.801728
-89.237865	-23.781318	1.806733
-89.718521	-14.451722	1.811738
-89.167931	-17.558408	1.816742
-89.895229	-15.570071	1.821747
-90.534561	-9.084463	1.826752
-90.715547	-14.579291	1.831757
-91.290740	-4.255326	1.836762
-90.959802	-9.889711	1.841766
-91.216747	-9.618724	1.846771
-91.370245	-6.892288	1.851776
-91.336913	-20.324955	1.856781
-92.296087	-11.909019	1.861786
-92.320075	-19.046127	1.866790
-92.388454	-20.620340	1.871795
-92.952842	-13.233789	1.876800
-92.584759	-22.089713	1.881805
-93.197026	-7.687910	1.886810
-93.849244	-14.584557	1.891814
-94.317694	-14.778490	1.896819
-94.369755	-13.264596	1.901824
-94.232467	-18.624187	1.906829
-94.520240	-12.552032	1.911834
-94.366497	-21.427088	1.916838
-94.455896	-13.526330	1.921843
-95.138789	-11.977234	1.926848
-95.376866	-15.989831	1.931853
-95.913618	-6.349179	1.936858
-95.590453	-10.448813	1.941862
-95.859699	-24.772521	1.946867
-96.797427	-5.978555	1.951872
-97.311071	-12.803792	1.956877
-97.564817	-3.619321	1.961882
-96.991008	-13.175358	1.966886
-97.464756	-12.043010	1.971891
-97.548421	-11.869226	1.976896
-97.298532	-19.063830	1.981901
-98.139183	-16.927719	1.986906
-98.991452	-15.082885	1.991910
-99.077799	-8.286757	1.996915
-99.235382	-13.246086	2.006912
-98.247244	-17.062827	2.016909
-97.913451	-13.622750	2.026906
-97.776804	-15.211453	2.036902
-97.710366	-8.680432	2.046899
-96.881038	-5.508104	2.056896
-96.575946	-9.467403	2.066893
-95.268818	-5.281687	2.076890
-94.784968	-9.306683	2.086886
-94.710873	-13.415436	2.096883
-94.612026	-9.899139	2.106880
-93.835833	-2.370788	2.116877
-93.491774	-11.271654	2.126874
-92.418563	-11.108601	2.136870
-91.871857	-6.015270	2.146867
-91.814670	-6.909115	2.156864
-91.564717	-6.367448	2.166861
-90.505299	-7.373492	2.176858
-90.354474	-10.269418	2.186854
-89.718370	-13.548206	2.196851
-88.877675	-8.814619	2.206848
-88.845658	-5.179557	2.216845
-88.228893	-16.756583	2.226842
-87.529695	-12.715319	2.236838
-87.387479	-16.168123	2.246835
-86.768735	-13.452716	2.256832
-86.250738	-12.046033	2.266829
-85.979551	-9.896978	2.276826
-84.943059	-14.521775	2.286822
-84.578520	-13.935826	2.296819
-84.354349	-9.203570	2.306816
-83.458218	-11.284069	2.316813
-83.020075	-12.744501	2.326810
-82.917133	-8.858457	2.336806
-82.334458	-11.164820	2.346803
-81.661785	-9.309755	2.356800
-81.352096	-9.789512	2.366797
-80.448887	-3.204061	2.376794
-79.852887	-4.080569	2.386790
-79.476650	-12.879478	2.396787
-79.559206	-15.217203	2.406784
-78.666039	-20.770891	2.416781
-78.206706	-11.104889	2.426778
-78.011261	-10.852033	2.436774
-76.678714	-19.514771	2.446771
-76.515458	-7.938730	2.456768
-76.482625	-9.376974	2.466765
-75.399876	-11.178985	2.476762
-74.834147	-11.778155	2.486758
-74.560448	-13.887654	2.496755
-74.642000	-10.869371	2.506752
-73.624692	-12.893242	2.516749
-73.411616	-12.135523	2.526746
-72.681278	-6.208810	2.536742
-71.559960	-12.953557	2.546739
-71.811907	-12.330274	2.556736
-71.345642	-1.295486	2.566733
-70.409285	-10.921887	2.576730
-70.336321	-15.703685	2.586726
-69.737072	-11.845977	2.596723
-69.039285	-4.751049	2.606720
-68.782257	-13.279160	2.616717
-68.104344	-8.397809	2.626714
-67.394686	-7.755744	2.636710
-67.065183	-9.087391	2.646707
-66.987543	-8.626248	2.656704
-65.940142	-7.679553	2.666701
-65.742839	-7.498224	2.676698
-65.348248	-8.205524	2.686694
-63.959691	-12.591276	2.696691
-63.913852	-9.882779	2.706688
-63.941216	-6.061975	2.716685
-63.645385	-12.867658	2.726682
-62.629138	-16.066038	2.736678
-62.150185	-15.733845	2.746675
-61.140625	-11.988052	2.756672
-60.826361	-5.738759	2.766669
-60.679123	-10.685498	2.776666
-60.431620	-11.005671	2.786662
-59.710739	-11.792627	2.796659
-59.309007	-16.896946	2.806656
-58.295419	-7.705012	2.816653
-57.809454	-6.133454	2.826650
-57.776129	-13.274376	2.836646
-57.257032	-11.639493	2.846643
-56.507293	-14.192903	2.856640
-56.188571	-12.282994	2.866637
-55.851768	-11.358041	2.876634
-54.893087	-10.501389	2.886630
-54.715542	-13.659199	2.896627
-54.041633	-12.870908	2.906624
-53.341310	-12.402188	2.916621
-52.948378	-19.837781	2.926618
-52.769546	-14.057684	2.936614
-52.278601	-19.847904	2.946611
-51.663536	-13.766712	2.956608
-51.275269	-12.527749	2.966605
-50.122531	-14.642551	2.976602
-49.726820	-14.431236	2.986598
-49.653164	-11.925340	2.996595
-49.591344	-10.213551	3.006592
-48.558350	-12.406998	3.016589
-48.158370	-16.258601	3.026586
-47.453435	-12.976066	3.036582
-46.730151	-14.920867	3.046579
-46.499791	-12.607756	3.056576
-46.637253	-6.696262	3.066573
-45.324688	-5.685864	3.076570
-44.911634	-9.805050	3.086566
-44.965045	-7.344977	3.096563
-43.767279	-18.069985	3.106560
-43.347234	-11.324619	3.116557
-43.300838	-10.733158	3.126554
-42.524578	-13.195677	3.136550
-41.844525	-11.239639	3.146547
-41.590459	-18.420991	3.156544
-41.323790	-14.760304	3.166541
-40.175657	-21.483644	3.176538
-40.059943	-18.021598	3.186534
-40.084868	-9.738040	3.196531
-38.614769	-9.932165	3.206528
-38.032757	-12.927650	3.216525
-38.123269	-17.170508	3.226522
-38.003647	-16.584975	3.236518
-37.422130	-17.384804	3.246515
-36.843789	-18.973405	3.256512
-35.731287	-20.651518	3.266509
-35.512311	-20.117768	3.276506
-35.375691	-18.390338	3.286502
-34.450704	-17.375697	3.296499
-34.040489	-17.793733	3.306496
-33.759278	-11.176209	3.316493
-32.575178	-8.761811	3.326490
-32.533826	-16.691284	3.336486
-32.389510	-6.930242	3.346483
-31.457940	-12.504006	3.356480
-30.936530	-17.134155	3.366477
-30.521302	-17.450535	3.376474
-30.180422	-17.183534	3.386470
-29.319795	-10.345224	3.396467
-28.877939	-18.342070	3.406464
-28.836325	-16.423012	3.416461
-27.863629	-18.480002	3.426458
-27.570132	-17.494007	3.436454
-27.156409	-12.636408	3.446451
-26.084817	-13.871549	3.456448
-25.812899	-16.687027	3.466445
-25.726059	-10.446969	3.476442
-25.453758	-15.122778	3.486438
-24.472148	-20.090498	3.496435
-24.118118	-14.113542	3.506432
-22.833882	-13.945394	3.516429
-23.195101	-10.049711	3.526426
-22.651014	-9.296464	3.536422
-22.133767	-17.024691	3.546419
-21.349496	-13.709578	3.556416
-20.784761	-6.607915	3.566413
-20.879663	-6.295518	3.576410
-19.569545	-16.486666	3.586406
-19.051815	-13.245102	3.596403
-18.978719	-11.952421	3.606400
-18.755406	-12.833714	3.616397
-18.358262	-16.285383	3.626394
-17.490503	-13.919805	3.636390
-17.189104	-16.713979	3.646387
-16.096840	-19.554590	3.656384
-16.065586	-11.700770	3.666381
-15.686659	-3.872891	3.676378
-14.853018	-12.233937	3.686374
-14.115787	-14.927320	3.696371
-14.100819	-13.297036	3.706368
-13.974237	-12.984889	3.716365
-12.972140	-9.507916	3.726362
-12.553620	-12.345350	3.736358
-11.735804	-7.913789	3.746355
-11.189901	-13.218701	3.756352
-11.183591	-18.483136	3.766349
-10.875203	-19.842752	3.776346
-9.904206	-17.730121	3.786342
-9.600984	-11.898813	3.796339
-8.849801	-10.401009	3.806336
-8.196577	-13.702970	3.816333
-8.029716	-14.051302	3.826330
-7.891740	-18.987916	3.836326
-6.822147	-11.887006	3.846323
-6.471677	-14.229075	3.856320
-6.041886	-16.826953	3.866317
-5.528837	-4.349850	3.876314
-4.883534	-4.438533	3.886310
-4.659523	-4.908030	3.896307
-3.825872	3.929013	3.906304
-3.824520	12.421065	3.916301
-3.120498	14.161070	3.926298
-2.676039	30.501802	3.936294
-2.482935	33.471941	3.946291
-1.976509	52.639120	3.956288
-1.337457	73.571637	3.966285
-1.076371	93.631193	3.976282
-0.785532	105.758729	3.986278
0.000000	107.676161	3.991283
-0.059270	124.546583	3.996288
0.139142	144.544993	4.001293
0.533440	154.798528	4.006298
0.368388	154.115729	4.011302
0.715666	153.414561	4.016307
0.700946	156.357526	4.021312
0.354136	157.129038	4.026317
0.865891	150.453505	4.031322
0.360819	162.813962	4.036326
0.975329	162.286263	4.041331
0.976314	172.137579	4.046336
0.775059	158.983043	4.051341
0.944343	158.988749	4.056346
0.867467	163.514737	4.061350
0.735860	147.661254	4.066355
0.936131	160.046124	4.071360
0.891928	173.277017	4.076365
1.223976	166.709210	4.081370
0.378576	162.350412	4.086374
0.848530	181.749756	4.091379
1.154772	178.618797	4.096384
0.929928	182.014787	4.101389
1.144904	181.875516	4.106394
0.878335	180.367081	4.111398
1.121076	177.499666	4.116403
1.462415	187.237527	4.121408
1.105100	173.538248	4.126413
1.040055	156.460800	4.131418
1.003281	169.150822	4.136422
0.905238	152.015298	4.141427
1.319810	170.093228	4.146432
0.925734	179.470886	4.151437
0.931629	165.410794	4.156442
1.070231	178.322918	4.161446
1.163884	180.338778	4.166451
1.368494	189.988743	4.171456
0.940570	178.688275	4.176461
1.531453	177.980588	4.181466
1.086456	176.714240	4.186470
0.943695	176.960831	4.191475
1.049466	186.363227	4.196480
1.083972	187.323985	4.201485
1.187196	190.030919	4.206490
1.199055	184.206799	4.211494
1.130557	186.753187	4.216499
1.269781	180.972046	4.221504
1.063835	186.118203	4.226509
1.683505	184.972862	4.231514
1.246542	190.244902	4.236518
1.089657	189.180537	4.241523
1.736198	191.139856	4.246528
1.315661	189.594021	4.251533
1.692612	195.589459	4.256538
1.448108	196.149420	4.261542
1.580735	186.130275	4.266547
1.628720	191.135421	4.271552
1.108916	193.030885	4.276557
1.536355	188.734515	4.281562
1.541661	196.996893	4.286566
1.608986	182.613307	4.291571
1.319224	180.262840	4.296576
1.081130	183.265119	4.301581
1.611734	183.216936	4.306586
1.560386	189.202253	4.311590
1.383563	191.961485	4.316595
1.206844	193.124172	4.321600
1.180441	189.300676	4.326605
1.325514	184.891939	4.331610
1.356136	192.857225	4.336614
1.090372	191.726602	4.341619
1.229488	186.909530	4.346624
1.431838	189.908774	4.351629
1.755688	199.280860	4.356634
1.655725	200.725249	4.361638
1.654936	192.635637	4.366643
1.482389	193.553267	4.371648
1.637917	211.044144	4.376653
1.664591	208.679066	4.381658
1.756851	223.202913	4.386662
1.909963	220.846436	4.391667
1.981969	205.607901	4.396672
1.512319	202.513508	4.401677
1.613270	198.591224	4.406682
1.775803	207.068835	4.411686
1.697674	210.933860	4.416691
1.955594	211.616093	4.421696
1.470235	199.380285	4.426701
1.836583	211.685562	4.431706
1.876215	221.510990	4.436710
2.027208	215.809775	4.441715
1.782655	226.518960	4.446720
1.599998	229.481011	4.451725
2.249611	225.988257	4.456730
1.867207	210.001340	4.461734
1.661077	199.593926	4.466739
1.762956	206.418933	4.471744
1.664995	216.345230	4.476749
2.086548	223.848252	4.481754
1.904959	225.511137	4.486758
1.959281	226.672542	4.491763
2.118157	230.136736	4.496768
2.068635	229.998063	4.501773
1.879457	221.251253	4.506778
1.745239	232.059903	4.511782
2.048172	226.748518	4.516787
1.875746	227.162102	4.521792
1.867027	221.811458	4.526797
2.403150	220.760621	4.531802
1.933425	231.531980	4.536806
2.201610	219.698839	4.541811
2.028617	223.690629	4.546816
1.898283	224.616773	4.551821
2.338471	223.874992	4.556826
1.896344	237.128094	4.561830
1.793577	216.914751	4.566835
2.147570	229.552677	4.571840
2.114090	232.453869	4.576845
2.092884	233.709048	4.581850
1.863079	232.945987	4.586854
2.288209	230.072394	4.591859
2.187794	224.045825	4.596864
1.695441	230.562092	4.601869
1.929451	212.459069	4.606874
1.797306	235.638890	4.611878
2.140919	253.927731	4.616883
2.555257	244.219520	4.621888
2.028828	254.228882	4.626893
2.602349	259.043220	4.631898
2.448970	257.462700	4.636902
2.737710	248.870609	4.641907
2.358898	249.187878	4.646912
2.291879	235.740581	4.651917
2.074335	236.229496	4.656922
2.306723	239.295310	4.661926
2.541432	251.479225	4.666931
2.555488	250.800662	4.671936
2.251696	259.470495	4.676941
2.524378	251.540073	4.681946
2.080572	264.137321	4.686950
2.315867	257.361518	4.691955
2.702504	253.642790	4.696960
2.627264	261.765302	4.701965
2.435832	250.676875	4.706970
2.536445	256.381392	4.711974
2.441774	255.246167	4.716979
2.356027	250.823860	4.721984
2.182075	260.425343	4.726989
2.256752	251.055512	4.731994
2.366165	256.380035	4.736998
2.563202	261.834610	4.742003
2.549509	256.185260	4.747008
2.611936	262.657608	4.752013
2.789502	252.836690	4.757018
2.536210	255.353941	4.762022
2.460764	258.192522	4.767027
2.578181	251.870383	4.772032
2.389859	258.937425	4.777037
2.479666	258.467034	4.782042
2.943524	247.610876	4.787046
2.706695	257.809055	4.792051
2.817009	261.930235	4.797056
2.998149	257.888038	4.802061
2.862500	257.271111	4.807066
2.810611	254.960444	4.812070
2.981294	260.046655	4.817075
2.944026	257.972810	4.822080
2.616309	261.951605	4.827085
2.948639	250.961502	4.832090
2.658583	255.289525	4.837094
2.752220	264.208492	4.842099
2.711551	259.291180	4.847104
2.494010	262.174849	4.852109
2.980584	247.924555	4.857114
2.941769	258.909935	4.862118
2.795345	252.548723	4.867123
2.812475	258.408016	4.872128
2.510852	265.389013	4.877133
2.927252	259.274458	4.882138
2.814036	263.206855	4.887142
2.883162	287.355435	4.892147
2.967792	285.933382	4.897152
2.719963	293.927275	4.902157
3.010936	294.266057	4.907162
3.079620	291.578031	4.912166
2.984141	289.426985	4.917171
3.240746	290.344338	4.922176
3.044685	295.382646	4.927181
3.105850	284.417304	4.932186
3.243008	298.720215	4.937190
3.285225	282.880782	4.942195
2.824222	264.600139	4.947200
2.815649	273.581482	4.952205
2.927289	276.972793	4.957210
2.945245	294.853300	4.962214
2.940297	285.547314	4.967219
3.027253	290.036992	4.972224
3.125158	298.406651	4.977229
3.075021	285.286819	4.982234
3.177272	297.306892	4.987238
3.070018	300.042512	4.992243
3.193192	294.432879	4.997248
3.007055	293.711137	5.002253
3.164798	293.936186	5.007258
3.118894	293.912143	5.012262
3.055441	293.610721	5.017267
3.086783	293.449213	5.022272
2.973262	298.643964	5.027277
3.010989	300.801675	5.032282
3.191877	314.252489	5.037286
3.423034	310.551352	5.042291
3.240686	321.359041	5.047296
3.227891	324.262258	5.052301
3.639963	306.157421	5.057306
3.357734	313.656728	5.062310
3.073347	317.069591	5.067315
3.632754	310.810926	5.072320
3.584653	320.033135	5.077325
3.320755	311.592220	5.082330
3.467093	322.540832	5.087334
3.779910	323.687446	5.092339
3.692817	314.747317	5.097344
3.766049	324.037972	5.102349
3.418375	297.163822	5.107354
3.486239	302.594476	5.112358
3.138241	298.761057	5.117363
3.294051	308.311627	5.122368
3.387024	323.994752	5.127373
3.569647	314.347875	5.132378
3.357936	318.310670	5.137382
3.172431	322.707068	5.142387
3.190093	320.884587	5.147392
3.187730	321.734835	5.152397
3.527393	322.985140	5.157402
3.180171	330.928589	5.162406
3.221470	334.550651	5.167411
3.785523	338.044002	5.172416
3.836564	345.137331	5.177421
4.012807	345.797552	5.182426
3.716948	347.082442	5.187430
3.391178	343.472050	5.192435
3.846744	341.824234	5.197440
4.088185	358.364347	5.202445
3.948725	330.256176	5.207450
3.697080	333.793661	5.212454
3.497948	320.616635	5.217459
3.842937	327.870134	5.222464
3.843558	340.512387	5.227469
3.582809	325.701838	5.232474
3.732691	331.439775	5.237478
4.043047	355.986432	5.242483
4.200452	348.408071	5.247488
3.633817	334.890927	5.252493
3.925165	334.983799	5.257498
3.657309	325.342892	5.262502
3.733611	341.498192	5.267507
3.794089	351.882990	5.272512
4.099538	366.592534	5.277517
4.380737	347.521239	5.282522
3.877367	339.215875	5.287526
3.903927	343.101812	5.292531
3.847748	327.141265	5.297536
3.819023	341.387969	5.302541
3.986283	349.742841	5.307546
4.250390	351.290650	5.312550
4.045148	364.480939	5.317555
4.271637	354.419438	5.322560
3.969424	340.862439	5.327565
3.657793	330.541232	5.332570
3.862735	343.530532	5.337574
3.949847	346.184021	5.342579
4.249754	355.379621	5.347584
3.944352	360.405930	5.352589
4.164369	356.312690	5.357594
4.215468	350.364325	5.362598
3.889568	360.381954	5.367603
4.204122	353.141069	5.372608
3.887935	362.996582	5.377613
3.792718	350.371897	5.382618
3.846705	354.920118	5.387622
4.182230	350.127956	5.392627
4.331622	352.452299	5.397632
3.720407	350.667542	5.402637
3.994771	341.150216	5.407642
4.341620	362.058944	5.412646
4.275711	358.761949	5.417651
4.452007	353.107507	5.422656
4.106900	365.039569	5.427661
4.171784	356.595992	5.432666
4.441847	363.191919	5.437670
4.194585	364.566745	5.442675
4.455148	362.048946	5.447680
3.941961	364.619621	5.452685
4.176635	373.340527	5.457690
4.405766	387.423117	5.462694
4.512935	384.955919	5.467699
4.840952	381.785509	5.472704
4.805012	378.977823	5.477709
4.542701	367.490616	5.482714
4.424911	363.161375	5.487718
4.081289	351.734281	5.492723
4.500942	368.840834	5.497728
4.519495	373.344405	5.502733
4.483278	369.997612	5.507738
4.385251	370.905601	5.512742
4.442714	376.903988	5.517747
4.646101	381.376720	5.522752
4.432150	381.533957	5.527757
4.609860	382.693038	5.532762
4.403520	381.394237	5.537766
4.391261	382.846741	5.542771
4.544216	376.253392	5.547776
4.655955	390.370775	5.552781
4.844417	372.200408	5.557786
4.529342	386.765581	5.562790
4.413359	381.935752	5.567795
4.665997	379.112046	5.572800
4.371906	380.914491	5.577805
4.519337	385.091032	5.582810
4.362699	385.727835	5.587814
4.578295	378.418250	5.592819
4.305412	379.910667	5.597824
4.335214	387.040575	5.602829
4.277260	388.962044	5.607834
4.603436	410.009314	5.612838
4.824422	410.526887	5.617843
4.917365	407.224447	5.622848
4.950029	422.651563	5.627853
5.036208	408.969350	5.632858
5.244047	421.569829	5.637862
4.985335	404.949415	5.642867
4.872329	386.332513	5.647872
4.610182	386.591240	5.652877
4.536377	381.344625	5.657882
4.550136	395.829419	5.662886
4.673571	419.892380	5.667891
5.261422	416.440868	5.672896
5.402410	417.267827	5.677901
5.248752	406.831770	5.682906
4.838268	388.601330	5.687910
4.617314	393.132451	5.692915
5.304220	397.760578	5.697920
4.872696	392.539038	5.702925
4.736811	392.436339	5.707930
4.734645	402.104429	5.712934
4.633332	409.750577	5.717939
5.310773	418.324643	5.722944
4.994297	418.858917	5.727949
5.199150	415.353692	5.732954
5.291000	418.347070	5.737958
5.010230	421.073798	5.742963
4.977869	408.045435	5.747968
4.990952	428.991851	5.752973
4.728758	420.045574	5.757978
4.847725	415.694260	5.762982
5.358818	420.437772	5.767987
5.126492	416.610563	5.772992
4.949789	419.022842	5.777997
4.809229	425.844109	5.783002
4.593973	414.226166	5.788006
4.967511	418.687759	5.793011
5.328896	427.650675	5.798016
5.145909	435.904934	5.803021
5.339604	440.191443	5.808026
5.630795	430.611002	5.813030
4.959090	418.280814	5.818035
5.260760	432.161841	5.823040
5.152054	443.493544	5.828045
5.107413	441.394946	5.833050
5.434237	450.109644	5.838054
5.314963	440.670133	5.843059
5.630913	438.034252	5.848064
5.410479	444.175864	5.853069
5.729281	428.583781	5.858074
5.184535	421.873277	5.863078
4.900089	428.730162	5.868083
5.566648	431.244600	5.873088
5.346988	439.890272	5.878093
5.456199	440.088519	5.883098
5.215903	439.061302	5.888102
5.380227	450.428097	5.893107
5.502480	436.780544	5.898112
5.115860	450.359199	5.903117
5.481002	444.834720	5.908122
5.608653	439.321274	5.913126
5.624752	457.938253	5.918131
5.635592	441.502729	5.923136
5.390309	450.911309	5.928141
5.426875	453.708428	5.933146
5.574028	443.755380	5.938150
5.699108	452.053153	5.943155
5.404949	452.675490	5.948160
5.227857	451.998811	5.953165
5.482849	448.487857	5.958170
5.078537	444.734740	5.963174
5.151076	446.441089	5.968179
5.525756	453.331915	5.973184
5.513266	470.486121	5.978189
5.536591	471.917856	5.983194
5.795256	482.512884	5.988198
5.968712	470.449156	5.993203
5.982489	477.389768	5.998208
5.767140	486.220327	6.003213
5.696854	468.605818	6.008218
5.752757	473.129686	6.013222
5.766097	472.736841	6.018227
5.648553	457.638199	6.023232
5.611410	467.047218	6.028237
5.710112	462.538628	6.033242
5.969144	465.701799	6.038246
5.768487	460.908136	6.043251
5.793607	437.229177	6.048256
5.476681	448.679742	6.053261
5.516634	453.061609	6.058266
5.849270	459.368336	6.063270
5.281141	467.936748	6.068275
5.741739	468.268616	6.073280
5.830281	481.550941	6.078285
6.072950	480.561606	6.083290
5.788733	466.279849	6.088294
5.379707	450.317206	6.093299
5.750262	465.057225	6.098304
5.975782	476.617652	6.103309
6.052539	447.146212	6.108314
5.798910	451.607179	6.113318
5.754344	451.635005	6.118323
5.697461	448.414240	6.123328
5.607644	439.920710	6.128333
5.678588	446.283799	6.133338
5.642213	443.974486	6.138342
5.552266	452.629609	6.143347
5.612820	447.068449	6.148352
5.537624	449.846548	6.153357
5.320975	440.018144	6.158362
5.672938	462.777153	6.163366
5.867687	473.143791	6.168371
6.077265	457.683972	6.173376
5.788892	453.696129	6.178381
5.740846	454.677551	6.183386
5.791693	438.876389	6.188390
5.466525	448.421587	6.193395
5.533343	431.130452	6.198400
5.693839	447.337655	6.203405
5.718045	458.627574	6.208410
5.667406	444.666939	6.213414
5.470163	454.051994	6.218419
5.582313	476.502397	6.223424
5.240429	474.112649	6.228429
5.931516	476.088126	6.233434
5.874856	476.528164	6.238438
5.747466	483.062755	6.243443
6.131009	477.966747	6.248448
5.674599	464.389837	6.253453
5.724208	458.140775	6.258458
5.794536	446.885923	6.263462
5.551779	449.428004	6.268467
5.629222	451.700718	6.273472
5.623655	466.041872	6.278477
5.854153	477.736539	6.283482
6.034039	464.883981	6.288486
5.798586	453.160921	6.293491
6.196509	452.343836	6.298496
5.359198	453.604955	6.303501
5.849224	453.487907	6.308506
6.016924	448.065608	6.313510
5.617245	451.203163	6.318515
5.937565	440.027562	6.323520
5.659036	452.630207	6.328525
5.655968	445.914726	6.333530
5.927790	442.172702	6.338534
5.537549	447.802531	6.343539
5.909663	441.950447	6.348544
5.539976	443.624708	6.353549
5.683298	439.155612	6.358554
5.748940	437.399378	6.363558
5.376027	450.838833	6.368563
5.577589	438.887689	6.373568
5.687488	434.523761	6.378573
5.791698	443.898357	6.383578
5.870338	440.680158	6.388582
5.784955	444.499184	6.393587
5.918916	448.295774	6.398592
5.851082	454.151227	6.403597
5.647546	435.328531	6.408602
5.925164	437.358913	6.413606
5.574726	449.847554	6.418611
5.901402	447.753890	6.423616
5.635356	450.878438	6.428621
5.598514	441.600813	6.433626
5.970870	429.945142	6.438630
5.565778	446.881058	6.443635
5.624829	438.480526	6.448640
5.572357	439.930309	6.453645
5.491287	446.490674	6.458650
5.826687	441.731849	6.463654
5.739069	437.583075	6.468659
5.790369	434.049651	6.473664
5.680532	446.933603	6.478669
5.544784	439.426630	6.483674
5.803205	440.476976	6.488678
5.653383	450.614635	6.493683
5.853782	443.144847	6.498688
5.497182	446.739756	6.503693
5.662296	449.233869	6.508698
6.051034	437.544211	6.513702
5.786984	452.997602	6.518707
5.512162	441.432396	6.523712
5.598556	448.214294	6.528717
5.618693	446.958959	6.533722
5.595475	441.667559	6.538726
5.547960	452.719233	6.543731
5.334836	444.107268	6.548736
5.486119	453.802617	6.553741
5.671326	448.560826	6.558746
5.593053	436.010026	6.563750
5.366046	456.427402	6.568755
5.750436	463.318995	6.573760
5.779770	471.797752	6.578765
5.818778	463.220076	6.583770
5.702766	457.153274	6.588774
5.500485	451.621736	6.593779
5.921806	470.364934	6.598784
5.531740	457.020057	6.603789
5.482700	462.386426	6.608794
5.920075	482.391958	6.613798
5.578082	475.849776	6.618803
5.885909	477.365511	6.623808
5.919869	479.794189	6.628813
5.673053	461.298262	6.633818
5.714909	452.563455	6.638822
5.223961	445.741349	6.643827
5.832921	462.443802	6.648832
6.031805	474.222320	6.653837
5.420802	470.508089	6.658842
5.731604	466.397055	6.663846
6.026162	465.788542	6.668851
5.736850	468.662701	6.673856
5.517158	458.645861	6.678861
5.510945	456.055719	6.683866
5.884079	456.333178	6.688870
5.909945	459.191260	6.693875
5.982858	444.499783	6.698880
6.015979	452.997831	6.703885
5.504180	445.143478	6.708890
6.020235	446.209161	6.713894
5.624811	450.895114	6.718899
5.616499	438.690576	6.723904
5.558890	446.966149	6.728909
5.548710	442.710064	6.733914
5.952700	445.331725	6.738918
5.490855	451.986193	6.743923
5.359711	443.739522	6.748928
5.448040	445.350524	6.753933
5.557626	469.608329	6.758938
5.802692	474.420781	6.763942
5.760672	485.462691	6.768947
5.770804	469.141104	6.773952
5.681889	468.556500	6.778957
5.792272	478.652361	6.783962
5.923523	453.132568	6.788966
5.554630	452.004366	6.793971
5.529989	445.830226	6.798976
5.465546	465.739208	6.803981
5.554036	473.983154	6.808986
5.973040	469.530350	6.813990
5.760005	476.134141	6.818995
5.788399	475.641139	6.824000
5.667636	464.940634	6.829005
6.004451	476.748943	6.834010
5.864866	461.940635	6.839014
5.413366	446.205019	6.844019
5.517401	451.685883	6.849024
5.805043	466.832751	6.854029
5.771004	458.265570	6.859034
5.723184	447.549965	6.864038
5.615773	465.714307	6.869043
5.952515	457.804171	6.874048
5.800282	456.082953	6.879053
5.627434	439.060396	6.884058
5.625411	441.314967	6.889062
5.494212	448.984522	6.894067
5.458432	450.891779	6.899072
5.524255	459.415503	6.904077
5.705126	478.175262	6.909082
5.705514	478.536419	6.914086
5.622475	484.240985	6.919091
5.811218	484.837191	6.924096
5.823743	477.043665	6.929101
5.811575	484.114454	6.934106
6.067267	475.546640	6.939110
5.868769	465.243248	6.944115
5.447544	453.850113	6.949120
5.845964	453.237756	6.954125
5.442948	452.477163	6.959130
5.555899	458.361442	6.964134
5.458654	472.797468	6.969139
5.937456	481.531070	6.974144
5.886713	476.362693	6.979149
5.600755	473.835746	6.984154
6.221498	466.289380	6.989158
5.566535	465.852776	6.994163
5.367531	457.756022	6.999168
5.602328	469.971174	7.004173
5.785268	471.682465	7.009178
5.865551	472.051630	7.014182
5.704606	468.978087	7.019187
5.669979	455.384165	7.024192
5.806345	459.855171	7.029197
5.668627	466.848043	7.034202
5.950549	439.806262	7.039206
5.757768	449.467505	7.044211
5.611715	444.140071	7.049216
5.918503	445.951253	7.054221
5.749979	451.961660	7.059226
5.677551	437.271813	7.064230
5.623002	450.345029	7.069235
5.678314	438.812678	7.074240
5.915024	447.172109	7.079245
5.434316	445.943899	7.084250
5.619944	450.619070	7.089254
5.183758	450.540543	7.094259
5.271614	469.660763	7.099264
5.927503	477.947486	7.104269
6.015676	477.236834	7.109274
5.938343	477.814660	7.114278
5.899424	474.882549	7.119283
5.712071	452.969507	7.124288
5.698904	461.715142	7.129293
5.648491	457.327089	7.134298
5.823391	447.392046	7.139302
5.965895	455.676680	7.144307
5.707768	449.520899	7.149312
5.931996	447.367016	7.154317
5.791818	440.653478	7.159322
5.904862	453.115744	7.164326
5.883990	444.588423	7.169331
5.740532	442.046910	7.174336
5.909566	455.391778	7.179341
5.775212	461.443897	7.184346
5.989070	451.493140	7.189350
6.103960	459.078624	7.194355
5.913253	459.038850	7.199360
5.799360	447.204253	7.204365
5.739449	451.769845	7.209370
5.897401	439.207924	7.214374
5.614081	433.801759	7.219379
5.748844	431.586007	7.224384
5.452696	429.465537	7.229389
5.475199	450.693766	7.234394
5.675678	449.658032	7.239398
5.604578	451.026345	7.244403
5.304424	455.296406	7.249408
5.329970	449.523888	7.254413
5.586687	455.874236	7.259418
5.615331	446.366769	7.264422
5.473636	450.269982	7.269427
5.506311	443.129898	7.274432
5.383461	444.867056	7.279437
5.550145	460.813686	7.284442
5.906224	450.150016	7.289446
5.541362	449.631534	7.294451
5.605653	443.046791	7.299456
5.790750	457.481822	7.304461
5.650236	452.076912	7.309466
5.662768	455.308934	7.314470
5.739022	458.103540	7.319475
5.754754	456.485285	7.324480
5.666784	459.267370	7.329485
5.464908	457.760548	7.334490
5.887970	467.947288	7.339494
5.272199	462.183471	7.344499
5.921579	478.414196	7.349504
6.094113	476.862172	7.354509
6.083563	459.892091	7.359514
5.995738	462.773302	7.364518
5.690857	457.091988	7.369523
5.974076	451.115288	7.374528
5.901874	448.395861	7.379533
5.496736	459.006846	7.384538
5.964931	451.825764	7.389542
5.857542	449.807284	7.394547
5.704546	438.687902	7.399552
5.837293	449.440946	7.404557
5.782431	461.710470	7.409562
5.674326	450.540449	7.414566
5.636731	456.317998	7.419571
5.686829	454.445056	7.424576
5.988643	447.639432	7.429581
5.859319	452.788505	7.434586
5.920693	448.222750	7.439590
6.027190	447.734699	7.444595
5.731828	445.863303	7.449600
5.787111	428.456774	7.454605
5.225596	429.084915	7.459610
5.756288	433.558229	7.464614
5.821689	443.842338	7.469619
5.530918	451.486174	7.474624
5.840881	448.484970	7.479629
5.558985	451.637492	7.484634
5.749559	448.498957	7.489638
5.727409	448.946216	7.494643
6.050870	448.364004	7.499648
5.938893	433.624462	7.504653
5.512902	430.732451	7.509658
5.630269	425.289670	7.514662
5.375443	428.206365	7.519667
5.536678	441.374929	7.524672
5.925659	448.667091	7.529677
5.663510	453.243019	7.534682
5.935835	448.419736	7.539686
5.881521	443.066586	7.544691
5.287545	434.026158	7.549696
5.724502	438.351194	7.554701
5.674116	447.196892	7.559706
5.608530	449.326414	7.564710
6.005046	455.117463	7.569715
5.666417	441.719112	7.574720
5.400628	447.173384	7.579725
5.169599	452.096964	7.584730
5.712695	451.050486	7.589734
5.455079	448.120584	7.594739
5.722249	452.386470	7.599744
5.678466	457.143850	7.604749
5.496280	451.390763	7.609754
5.808525	453.888581	7.614758
5.684098	448.737915	7.619763
5.676645	447.866571	7.624768
5.768006	451.920888	7.629773
5.652214	454.316595	7.634778
5.567100	451.332535	7.639782
5.740605	459.342322	7.644787
5.312591	442.405436	7.649792
5.919656	448.385440	7.654797
5.822502	452.926900	7.659802
5.885822	440.616898	7.664806
5.567350	453.449502	7.669811
5.510689	446.853570	7.674816
5.661657	446.151682	7.679821
5.903582	456.365093	7.684826
5.242302	458.784649	7.689830
5.428412	449.934352	7.694835
5.674960	464.974851	7.699840
5.890382	452.494876	7.704845
5.697653	453.759772	7.709850
5.635778	460.342720	7.714854
5.812629	453.526866	7.719859
5.732153	448.153373	7.724864
5.850151	454.386256	7.729869
5.615737	453.723982	7.734874
5.449095	450.326707	7.739878
5.834120	456.575545	7.744883
5.703653	449.702153	7.749888
5.567874	444.320733	7.754893
5.410671	451.251212	7.759898
5.390340	454.218544	7.764902
5.542442	470.668669	7.769907
5.934004	480.927611	7.774912
6.022243	484.274296	7.779917
5.538968	462.628766	7.784922
5.484750	455.850208	7.789926
5.995112	484.410211	7.794931
5.902050	464.841336	7.799936
6.161078	457.297134	7.804941
5.799904	461.744009	7.809946
6.283864	444.112717	7.814950
6.131320	457.575547	7.819955
5.881125	462.110336	7.824960
5.773787	447.860632	7.829965
5.897486	451.373013	7.834970
5.912720	451.150433	7.839974
5.598568	445.283208	7.844979
5.778881	455.292716	7.849984
6.015864	441.168039	7.854989
5.501825	447.104034	7.859994
5.660242	443.111912	7.864998
5.469849	445.316320	7.870003
5.303053	450.788863	7.875008
5.840019	451.193447	7.880013
5.578879	449.283543	7.885018
5.649833	459.470456	7.890022
5.603606	455.456408	7.895027
5.895272	456.030672	7.900032
6.024400	455.796669	7.905037
5.585566	457.011866	7.910042
5.746557	457.595787	7.915046
5.538867	453.382303	7.920051
5.879259	453.693487	7.925056
5.821291	456.915061	7.930061
5.624944	460.784590	7.935066
5.711773	454.912362	7.940070
5.785231	461.464166	7.945075
5.601217	454.803346	7.950080
6.010343	448.204530	7.955085
5.505462	451.618839	7.960090
5.833186	447.135644	7.965094
5.795722	452.713490	7.970099
5.726770	448.588561	7.975104
5.758782	443.254589	7.980109
5.603522	448.359210	7.985114
5.592869	451.856206	7.990118
5.574629	445.118248	7.995136
5.493949	458.729076	8.000154
5.509481	450.663764	8.005171
5.457304	465.750976	8.010189
5.523620	459.222320	8.015206
5.909851	451.458565	8.020224
5.746581	465.305737	8.025242
5.791948	446.332159	8.030259
5.747272	454.201226	8.035277
6.021759	447.938898	8.040294
6.049805	464.301657	8.045312
5.901048	454.403840	8.050330
5.983749	447.455246	8.055347
5.920314	450.887199	8.060365
5.944759	448.459494	8.065382
5.969415	433.271733	8.070400
5.724458	429.237224	8.075418
5.847587	423.563777	8.080435
5.562022	425.707023	8.085453
5.777061	419.072131	8.090470
5.598407	431.184780	8.095488
5.712850	448.241658	8.100506
5.970211	446.074121	8.105523
5.917970	455.196539	8.110541
5.706633	442.336366	8.115558
5.892157	454.740942	8.120576
5.934055	453.464147	8.125594
6.000311	444.634609	8.130611
5.569904	437.810666	8.135629
5.937566	443.985157	8.140646
5.988516	444.149577	8.145664
5.620086	441.681406	8.150682
5.902454	443.576798	8.155699
6.087325	450.591270	8.160717
5.493183	445.402904	8.165734
5.964759	448.221947	8.170752
5.754913	449.213159	8.175770
5.713506	446.546684	8.180787
5.549286	455.612328	8.185805
5.691400	447.331357	8.190822
5.744643	446.094410	8.195840
5.794019	456.936682	8.200858
6.049557	452.588010	8.205875
5.907691	458.091060	8.210893
5.932955	455.378632	8.215910
6.339589	448.287449	8.220928
5.886464	455.625617	8.225946
6.181507	454.747152	8.230963
6.084164	450.056978	8.235981
6.060886	449.431174	8.240998
6.518016	457.233062	8.246016
6.065161	449.327223	8.251034
5.774182	446.274227	8.256051
5.512736	445.371312	8.261069
5.828025	457.682316	8.266086
6.038506	449.819680	8.271104
5.980224	456.291290	8.276122
6.143064	462.707467	8.281139
6.091962	459.895969	8.286157
5.936094	456.944533	8.291174
6.022414	464.928839	8.296192
5.457797	456.959397	8.301210
5.899793	453.552347	8.306227
6.200579	456.254075	8.311245
5.852854	462.134479	8.316262
5.709215	455.010928	8.321280
5.810598	457.559722	8.326298
6.010465	457.644228	8.331315
5.974072	469.871952	8.336333
5.992869	458.295113	8.341350
5.981676	456.588009	8.346368
5.885815	464.326003	8.351386
6.241074	459.624798	8.356403
6.166043	464.675755	8.361421
6.084437	460.546148	8.366438
5.850149	453.109595	8.371456
5.727103	451.950884	8.376474
5.952751	466.888270	8.381491
5.965721	473.392788	8.386509
6.196340	474.417489	8.391526
6.365827	477.941934	8.396544
5.819300	489.935932	8.401562
6.084776	474.198695	8.406579
5.979822	487.579750	8.411597
6.035437	487.852530	8.416614
6.147628	478.971099	8.421632
6.313699	483.364532	8.426650
6.288952	480.019650	8.431667
6.412829	498.415988	8.436685
6.172943	485.422041	8.441702
6.215356	487.514343	8.446720
6.344958	487.665273	8.451738
6.176206	478.233346	8.456755
6.530536	488.818496	8.461773
5.969824	477.959722	8.466790
6.195079	479.775009	8.471808
6.254863	495.425321	8.476826
6.438124	477.282776	8.481843
6.201423	475.733875	8.486861
6.149968	465.320863	8.491878
6.138464	458.500898	8.496896
5.988897	471.045590	8.501914
6.257392	481.359644	8.506931
6.266668	478.946151	8.511949
6.157261	488.864881	8.516966
6.248277	494.042904	8.521984
6.134660	483.700769	8.527002
6.087518	489.883603	8.532019
6.294941	490.163376	8.537037
5.894809	488.513457	8.542054
6.269000	492.293683	8.547072
6.028352	496.086950	8.552090
6.181669	487.901723	8.557107
6.568393	488.486835	8.562125
5.920995	492.046299	8.567143
6.223631	489.552244	8.572160
5.907779	487.018401	8.577178
6.333808	483.400346	8.582195
6.252788	486.996204	8.587213
6.360785	491.966737	8.592231
6.242069	492.063841	8.597248
6.135267	495.164360	8.602266
6.003897	488.273559	8.607283
6.216110	508.892546	8.612301
6.104292	524.218956	8.617319
6.391668	519.803402	8.622336
6.435810	527.570938	8.627354
6.548721	522.383591	8.632371
6.591779	519.031825	8.637389
6.381006	530.998120	8.642407
7.015160	522.454927	8.647424
6.480153	511.728467	8.652442
6.122632	502.939209	8.657459
6.335463	493.111409	8.662477
6.598307	508.001752	8.667495
6.400088	505.890009	8.672512
6.345968	508.129539	8.677530
6.502002	514.968627	8.682547
6.537399	505.678009	8.687565
6.218897	511.943877	8.692583
6.759561	517.919568	8.697600
6.597400	519.078360	8.702618
6.611011	496.059124	8.707635
6.434516	492.136685	8.712653
6.376025	490.311730	8.717671
6.589138	486.437089	8.722688
6.302488	490.701641	8.727706
6.302274	494.372121	8.732723
6.649571	494.875775	8.737741
6.528583	520.268062	8.742759
6.744615	500.326642	8.747776
6.367776	483.161999	8.752794
6.417618	492.182646	8.757811
6.335979	508.042130	8.762829
6.389320	511.602309	8.767847
6.416489	516.851704	8.772864
6.216376	512.984137	8.777882
6.295347	508.496159	8.782899
6.437290	519.458385	8.787917
6.285489	518.479682	8.792935
6.429756	509.491182	8.797952
6.703126	519.119951	8.802970
6.412145	509.687637	8.807987
6.806133	516.014862	8.813005
6.647402	517.400796	8.818023
7.080384	514.416297	8.823040
6.634039	516.263849	8.828058
6.887378	513.812183	8.833075
6.850618	511.921541	8.838093
6.478525	514.043378	8.843111
6.554694	502.795144	8.848128
6.694859	517.089459	8.853146
6.680643	514.060580	8.858163
6.510002	518.975221	8.863181
6.435600	519.244098	8.868199
6.808888	514.026420	8.873216
6.605248	518.692235	8.878234
6.516197	511.646823	8.883251
6.753125	520.820293	8.888269
6.341019	518.806578	8.893287
6.436945	511.600113	8.898304
6.370449	520.306704	8.903322
6.164099	519.828745	8.908339
6.645486	533.148566	8.913357
6.892858	540.376525	8.918375
6.817279	542.746450	8.923392
6.719321	527.820935	8.928410
6.934713	527.673199	8.933427
7.019266	514.568241	8.938445
6.734311	510.839571	8.943463
6.700707	516.927088	8.948480
6.717586	514.319656	8.953498
6.546532	520.179251	8.958515
6.608716	515.443899	8.963533
6.893376	529.661109	8.968551
6.661886	523.885040	8.973568
6.779952	530.987246	8.978586
6.626190	541.752048	8.983603
7.097910	548.185805	8.988621
7.257152	542.670191	8.993639
6.872662	528.163112	8.998656
6.602505	525.780241	9.003674
6.678274	512.107366	9.008691
6.746522	511.743936	9.013709
6.533784	523.176407	9.018727
6.858410	538.410434	9.023744
7.007592	541.117254	9.028762
7.029961	549.013964	9.033779
6.944145	536.108860	9.038797
6.908586	531.600735	9.043815
6.699916	522.991451	9.048832
6.922330	526.560496	9.053850
6.697895	534.499460	9.058867
7.125060	539.531809	9.063885
6.849861	544.629451	9.068903
6.984663	526.054789	9.073920
7.277458	525.872711	9.078938
7.032346	529.250076	9.083955
7.094820	512.272001	9.088973
6.754378	515.409757	9.093991
6.662667	518.454844	9.099008
6.741911	518.817697	9.104026
6.708307	526.181433	9.109043
7.078382	533.330067	9.114061
7.011998	544.260217	9.119079
7.030428	541.057074	9.124096
7.340135	545.080205	9.129114
6.837450	533.712002	9.134131
6.882525	519.806346	9.139149
7.046316	530.846155	9.144167
7.008360	532.042874	9.149184
6.962947	534.966755	9.154202
7.030827	536.276569	9.159219
7.101969	535.676291	9.164237
7.024401	529.576419	9.169255
6.887912	537.778255	9.174272
6.986072	540.585122	9.179290
7.019809	548.484775	9.184307
7.225317	548.797634	9.189325
6.958853	544.806602	9.194343
7.244552	543.573154	9.199360
7.078534	535.260592	9.204378
6.968623	541.317037	9.209395
7.153212	552.109969	9.214413
7.350662	550.274398	9.219431
7.036373	528.938891	9.224448
7.157639	520.027105	9.229466
6.792599	520.235668	9.234483
6.910101	529.788648	9.239501
6.949941	551.410487	9.244519
6.923373	546.200226	9.249536
7.255633	537.107922	9.254554
7.320247	551.023199	9.259571
7.417510	545.141820	9.264589
6.912380	545.134606	9.269607
7.220550	539.203319	9.274624
7.126700	541.341862	9.279642
7.055016	541.320291	9.284659
7.136821	541.632632	9.289677
7.169645	544.534827	9.294695
7.262495	546.934093	9.299712
7.654600	544.792001	9.304730
7.300491	551.566227	9.309747
7.131611	548.389706	9.314765
7.516901	546.682905	9.319783
7.226063	544.688115	9.324800
7.184206	533.769635	9.329818
6.971645	539.989174	9.334835
7.380592	546.464893	9.339853
7.342620	552.629705	9.344871
7.203659	538.096606	9.349888
7.419915	531.216534	9.354906
7.387321	540.718651	9.359923
7.101475	528.131197	9.364941
6.770318	536.022851	9.369959
7.058921	528.792803	9.374976
7.360483	540.053305	9.379994
6.985979	546.146785	9.385011
7.107483	549.474690	9.390029
7.143802	559.524372	9.395047
7.054515	551.239960	9.400064
7.495297	544.255961	9.405082
7.366199	553.062268	9.410099
7.308700	543.831753	9.415117
7.033320	547.129300	9.420135
7.241965	549.228483	9.425152
7.374171	533.630410	9.430170
7.420842	556.707622	9.435187
7.010753	548.764848	9.440205
7.540561	538.969462	9.445223
7.254735	539.749855	9.450240
7.628707	541.952104	9.455258
7.231481	542.912586	9.460275
7.531595	535.150622	9.465293
7.382464	539.058769	9.470311
7.094596	541.178303	9.475328
7.287794	553.761478	9.480346
7.641945	573.393413	9.485363
7.454840	564.649958	9.490381
7.660703	561.872929	9.495399
7.361663	574.379328	9.500416
7.515638	544.621737	9.505434
7.390889	561.195737	9.510451
7.736101	562.468776	9.515469
7.619118	552.441359	9.520487
7.096320	548.576134	9.525504
7.599334	552.419320	9.530522
7.487115	560.217928	9.535539
7.606098	565.292750	9.540557
7.721668	556.717053	9.545575
7.440617	559.354747	9.550592
7.530320	548.177654	9.555610
7.286197	552.767313	9.560627
7.165442	567.437600	9.565645
7.502118	568.404631	9.570663
7.484868	569.173903	9.575680
7.805836	571.290741	9.580698
7.516829	580.558639	9.585715
7.708185	582.215006	9.590733
7.563433	579.965013	9.595751
7.495173	577.626805	9.600768
7.644610	577.076469	9.605786
7.506363	584.431940	9.610803
7.484895	574.843161	9.615821
7.602937	583.738146	9.620839
7.872303	581.889211	9.625856
7.952211	574.386604	9.630874
7.918334	580.250614	9.635891
7.813950	576.654456	9.640909
7.979675	557.010096	9.645927
7.736819	553.776128	9.650944
7.716248	544.264763	9.655962
7.543746	548.329697	9.660979
7.352229	541.326199	9.665997
7.749930	551.920758	9.671015
7.442167	562.330293	9.676032
7.694932	570.480121	9.681050
7.934548	570.638654	9.686067
7.579907	566.254297	9.691085
7.964597	571.998258	9.696103
7.786834	573.665928	9.701120
7.816253	557.799932	9.706138
7.671474	554.634385	9.711155
7.538455	564.278579	9.716173
7.914316	565.852496	9.721191
7.579152	566.732462	9.726208
7.653039	563.568073	9.731226
7.540649	581.195942	9.736243
7.664371	569.042442	9.741261
7.857034	572.226926	9.746279
7.458217	578.150555	9.751296
7.761875	575.867496	9.756314
8.034428	570.305691	9.761331
7.715134	566.122932	9.766349
7.937719	574.219690	9.771367
7.946250	571.819197	9.776384
7.888266	575.922977	9.781402
7.576020	570.952694	9.786419
7.796334	572.121202	9.791437
8.343338	571.208867	9.796455
7.985385	562.272530	9.801472
7.872794	566.006864	9.806490
8.020210	572.986744	9.811507
8.289471	572.254139	9.816525
8.317832	576.655300	9.821543
7.990157	550.077459	9.826560
7.813209	541.735800	9.831578
7.928839	552.211061	9.836595
7.717141	561.108272	9.841613
7.805104	556.874844	9.846631
7.782235	566.955666	9.851648
7.850463	577.151631	9.856666
7.891749	573.294146	9.861683
7.544644	587.162360	9.866701
7.870772	576.995080	9.871719
7.566178	583.239883	9.876736
7.535448	575.243654	9.881754
7.672358	571.021520	9.886771
7.533019	588.166546	9.891789
8.141084	592.680041	9.896807
8.478459	606.627443	9.901824
8.088699	594.199796	9.906842
7.990584	578.074891	9.911859
8.117206	580.031070	9.916877
7.784424	566.773622	9.921895
7.804438	588.128667	9.926912
8.145273	601.140247	9.931930
8.522602	601.449413	9.936947
8.060931	594.292543	9.941965
8.200643	587.262037	9.946983
7.965339	580.243223	9.952000
7.869032	580.521626	9.957018
7.996079	599.858219	9.962035
7.932283	609.578681	9.967053
8.132449	606.341359	9.972071
8.266901	604.888362	9.977088
8.470141	607.363471	9.982106
8.494799	615.461076	9.987123
8.060835	595.194948	9.992141
8.161425	581.241684	9.997159
8.052435	576.968766	10.002176
8.383693	581.521112	10.007194
8.347373	576.410366	10.012211
8.002227	583.480112	10.017229
8.383086	572.219165	10.022247
8.023605	576.764226	10.027264
7.955674	569.938186	10.032282
8.358906	589.861478	10.037299
8.511018	593.553651	10.042317
8.312671	583.338617	10.047335
8.150106	579.844771	10.052352
8.048750	570.224619	10.057370
8.372473	592.255613	10.062387
8.026737	590.969159	10.067405
8.569030	593.686994	10.072423
8.472863	592.794348	10.077440
8.315778	576.530598	10.082458
8.277857	573.046464	10.087475
8.070313	579.479222	10.092493
8.358522	570.934621	10.097511
8.151097	588.831498	10.102528
8.325263	592.606819	10.107546
8.489205	585.553417	10.112563
7.880939	603.188862	10.117581
8.497151	598.709595	10.122599
8.374348	606.112121	10.127616
8.218028	614.530028	10.132634
8.544200	613.550071	10.137651
8.508351	605.490709	10.142669
8.805486	599.854471	10.147687
8.432924	594.068525	10.152704
8.200465	580.983031	10.157722
8.446483	588.988934	10.162739
8.520339	600.228658	10.167757
8.329514	576.542831	10.172775
8.441676	599.769785	10.177792
8.477054	603.269776	10.182810
8.741992	601.273077	10.187827
8.253963	599.436629	10.192845
8.571881	588.788117	10.197863
7.894037	595.080337	10.202880
8.522516	595.622256	10.207898
8.581599	600.690949	10.212915
8.541527	622.480295	10.217933
8.778729	605.720044	10.222951
8.533502	615.809008	10.227968
8.381285	618.967145	10.232986
8.440780	604.430021	10.238003
8.383275	598.876302	10.243021
8.749941	602.739869	10.248039
8.657707	601.471548	10.253056
8.196270	606.082374	10.258074
8.570471	605.866965	10.263091
8.483516	606.491686	10.268109
8.627072	615.332385	10.273127
8.527917	599.665610	10.278144
8.510953	600.001852	10.283162
8.748945	606.131512	10.288179
8.683468	609.146205	10.293197
8.418065	602.110705	10.298215
8.818761	609.446501	10.303232
8.938634	595.468881	10.308250
8.745967	602.010487	10.313267
8.576433	608.115484	10.318285
8.735427	598.988699	10.323303
8.760849	608.002330	10.328320
8.462215	603.302075	10.333338
8.224461	601.430467	10.338355
8.593840	610.594108	10.343373
8.301438	593.580020	10.348391
8.533603	606.783740	10.353408
8.376028	600.671771	10.358426
8.341140	597.697954	10.363443
8.380846	615.376892	10.368461
8.793019	634.994102	10.373479
8.816342	624.697634	10.378496
8.820246	637.601374	10.383514
9.071611	631.763970	10.388531
8.842042	643.011257	10.393549
8.833839	624.810334	10.398567
8.734391	614.532882	10.403584
8.371590	615.970261	10.408602
8.733915	621.147479	10.413619
8.636634	633.429087	10.418637
8.556950	633.723539	10.423655
9.056719	634.993381	10.428672
9.010992	644.773663	10.433690
9.335108	628.885070	10.438707
8.879052	636.505838	10.443725
8.917703	637.599177	10.448743
8.977742	633.563612	10.453760
9.187471	631.152001	10.458778
9.058825	614.068121	10.463795
8.861931	601.491197	10.468813
8.818440	603.097712	10.473831
8.904489	597.617692	10.478848
8.690190	610.773764	10.483866
9.277724	611.147386	10.488883
8.853951	612.126430	10.493901
8.749844	607.313237	10.498919
8.977100	611.047906	10.503936
8.664341	623.120576	10.508954
9.003480	628.176849	10.513971
9.150145	629.914509	10.518989
9.331618	632.350609	10.524007
9.320938	608.169996	10.529024
9.048253	604.987001	10.534042
8.816290	603.751120	10.539059
8.851220	597.880021	10.544077
8.996676	601.449697	10.549095
8.999502	603.704432	10.554112
8.891404	619.454351	10.559130
9.186002	623.722472	10.564147
9.156347	639.938193	10.569165
8.724245	636.469982	10.574183
8.917403	627.741589	10.579200
9.318327	632.500308	10.584218
9.185396	630.205155	10.589235
9.301338	628.403316	10.594253
9.262521	633.776036	10.599271
9.456425	620.088757	10.604288
8.651124	623.446633	10.609306
9.227641	622.007671	10.614323
9.371589	614.942010	10.619341
8.908540	619.279539	10.624359
9.231147	617.800073	10.629376
9.034851	627.924847	10.634394
9.424757	634.225734	10.639411
9.465733	633.071985	10.644429
9.211016	633.450272	10.649447
9.379470	608.395439	10.654464
9.259171	614.717160	10.659482
8.983211	597.991434	10.664499
9.069087	605.057271	10.669517
9.250919	630.238213	10.674535
9.518817	624.395619	10.679552
9.427444	619.749870	10.684570
9.330219	612.483956	10.689587
8.989503	603.429218	10.694605
9.355171	617.739992	10.699623
9.278539	617.717074	10.704640
9.212153	634.072789	10.709658
9.396949	630.357387	10.714675
9.258769	626.283827	10.719693
9.232009	632.848806	10.724711
9.307525	626.898365	10.729728
9.436626	631.799033	10.734746
9.095246	643.689084	10.739763
9.118176	635.422000	10.744781
9.316038	635.039510	10.749799
9.278189	633.999554	10.754816
9.141321	641.975077	10.759834
9.564395	650.024475	10.764851
9.423513	639.197073	10.769869
9.371292	634.887892	10.774887
9.312631	634.275603	10.779904
9.224144	635.147283	10.784922
9.279341	639.404980	10.789939
9.338281	637.353458	10.794957
9.005581	639.122314	10.799975
9.307401	639.628274	10.804992
9.132459	640.528903	10.810010
9.568223	651.043830	10.815027
9.501400	663.913422	10.820045
9.400848	664.561059	10.825063
9.946691	665.256373	10.830080
9.428195	658.690935	10.835098
9.597022	637.058061	10.840115
9.507798	637.450331	10.845133
9.321036	651.634066	10.850151
9.658898	650.969337	10.855168
9.882940	661.648171	10.860186
9.758103	635.921429	10.865203
9.802502	635.324583	10.870221
9.765464	635.447847	10.875239
9.819139	622.550714	10.880256
9.804351	622.779728	10.885274
9.637478	627.565263	10.890291
9.683653	623.319337	10.895309
9.228411	628.429834	10.900327
9.713409	624.327489	10.905344
9.549271	636.773268	10.910362
9.671478	622.608758	10.915379
9.307042	628.275888	10.920397
9.322640	640.529892	10.925415
9.887355	634.165207	10.930432
9.693333	655.519404	10.935450
9.363660	656.051587	10.940467
9.649907	653.193850	10.945485
9.776535	661.204957	10.950503
9.987470	655.532462	10.955520
9.777783	665.686831	10.960538
9.561860	660.564702	10.965555
10.097478	660.960091	10.970573
9.749617	664.164542	10.975591
9.892732	658.360073	10.980608
9.839284	677.923994	10.985626
9.612365	655.007150	10.990643
9.878067	655.842637	10.995661
9.763683	669.790456	11.000679
9.739303	661.103799	11.005696
9.660705	659.432905	11.010714
9.789704	662.894806	11.015731
9.901531	660.947707	11.020749
9.712000	659.066942	11.025767
9.833180	666.239549	11.030784
10.149710	660.251924	11.035802
9.972577	670.213059	11.040819
9.627352	667.030525	11.045837
9.567757	668.629769	11.050855
9.708567	667.754541	11.055872
9.880229	671.337911	11.060890
9.920707	666.632965	11.065907
10.103322	656.332392	11.070925
9.883371	672.627420	11.075943
10.028459	660.324873	11.080960
10.085332	672.890820	11.085978
9.684521	667.311541	11.090995
9.976216	653.968238	11.096013
10.058998	661.892515	11.101031
9.791236	657.469862	11.106048
10.010653	664.788408	11.111066
9.720758	665.825827	11.116083
9.904445	656.293627	11.121101
9.948087	675.188774	11.126119
9.983838	657.545498	11.131136
10.088612	664.052540	11.136154
10.337005	675.004668	11.141171
10.580618	666.719204	11.146189
10.187320	673.522297	11.151207
10.017875	660.031419	11.156224
10.126122	659.840376	11.161242
9.718827	674.134971	11.166259
9.881533	659.065583	11.171277
10.388872	667.216200	11.176295
9.956959	675.579703	11.181312
10.197817	671.786340	11.186330
9.990181	675.323653	11.191347
10.383567	682.097220	11.196365
10.469222	679.128757	11.201383
10.262780	669.690050	11.206400
10.266482	663.119893	11.211418
10.045334	665.276636	11.216435
10.077003	658.285208	11.221453
9.941753	658.385635	11.226471
10.090523	679.426771	11.231488
10.569178	686.372826	11.236506
10.466392	691.201225	11.241523
10.515248	679.065816	11.246541
10.288508	675.337916	11.251559
10.206283	668.953970	11.256576
10.294937	667.822747	11.261594
10.569623	672.753492	11.266611
10.733123	659.513538	11.271629
10.486757	661.913476	11.276647
10.254492	664.960269	11.281664
10.478825	672.168381	11.286682
10.133718	661.786443	11.291699
10.011092	660.624892	11.296717
10.116235	664.021458	11.301735
10.466722	679.483787	11.306752
10.518985	690.261586	11.311770
10.291574	683.401329	11.316787
10.545363	683.146479	11.321805
10.820738	684.642151	11.326823
10.309358	670.322508	11.331840
10.270275	654.880546	11.336858
10.382155	681.409485	11.341875
10.603321	687.672937	11.346893
10.703307	681.974287	11.351911
10.557007	680.470946	11.356928
10.416799	659.209915	11.361946
10.417500	676.329831	11.366963
10.455286	675.383750	11.371981
10.284919	682.590866	11.376999
10.548008	691.534469	11.382016
10.399178	678.870126	11.387034
10.417983	682.118298	11.392051
10.609483	688.664847	11.397069
10.210553	684.381457	11.402087
10.645355	688.382380	11.407104
10.820784	679.559267	11.412122
10.589872	683.906671	11.417139
10.804731	682.977283	11.422157
10.317355	687.002475	11.427175
10.190873	688.174375	11.432192
10.222443	676.547830	11.437210
10.180870	685.775393	11.442227
10.332046	685.624097	11.447245
10.957089	704.625327	11.452263
10.883318	704.732422	11.457280
10.589994	684.324748	11.462298
10.818644	681.003978	11.467315
10.862744	685.804657	11.472333
10.602905	681.339947	11.477351
10.672218	681.757486	11.482368
10.608736	689.405711	11.487386
10.796135	701.688646	11.492403
11.026899	711.915802	11.497421
10.691740	704.484675	11.502439
11.003708	701.104570	11.507456
10.973887	683.114591	11.512474
10.824022	686.215179	11.517491
10.700868	683.779846	11.522509
10.624790	689.136601	11.527527
10.776219	700.727386	11.532544
11.242178	704.898623	11.537562
10.912344	690.515698	11.542579
11.020753	679.871929	11.547597
11.264390	688.300539	11.552615
10.802280	682.117035	11.557632
10.773880	676.171152	11.562650
10.670528	683.293389	11.567667
10.663002	678.420914	11.572685
10.928446	686.190928	11.577703
11.156996	703.600717	11.582720
11.174403	676.424395	11.587738
10.911986	681.288027	11.592755
10.847996	682.527833	11.597773
10.942414	688.455804	11.602791
11.064686	697.804202	11.607808
11.063293	689.381887	11.612826
10.932690	688.501126	11.617843
10.753514	694.698777	11.622861
10.873393	710.542684	11.627879
10.965767	707.922743	11.632896
11.038541	699.268720	11.637914
10.998693	716.729372	11.642931
10.728508	719.804682	11.647949
10.949550	709.826105	11.652967
11.245147	719.925842	11.657984
11.376302	712.464001	11.663002
11.428262	720.990335	11.668019
11.439958	715.228423	11.673037
11.520193	702.287571	11.678055
11.192715	709.060121	11.683072
11.371528	701.173068	11.688090
11.055441	702.013282	11.693107
11.188889	690.439660	11.698125
11.287087	703.242260	11.703143
11.182821	698.030518	11.708160
11.107296	685.800917	11.713178
11.253836	698.098179	11.718195
11.223182	698.757686	11.723213
11.798664	710.385567	11.728231
11.198078	702.967995	11.733248
11.171069	676.252076	11.738266
10.919072	685.904593	11.743283
11.178606	701.512756	11.748301
11.421530	704.004252	11.753319
11.551197	710.122923	11.758336
11.581515	711.240081	11.763354
11.295111	698.689087	11.768371
10.942247	678.204761	11.773389
11.280002	705.144457	11.778407
11.397899	712.346560	11.783424
11.416378	712.739435	11.788442
11.294352	721.513967	11.793459
11.136173	714.082127	11.798477
11.621281	712.053458	11.803495
11.155355	730.312744	11.808512
11.318156	718.771251	11.813530
11.253905	713.706504	11.818547
11.241591	715.132026	11.823565
11.410681	710.491722	11.828583
11.236898	723.191477	11.833600
11.629287	718.717478	11.838618
11.413788	717.098034	11.843635
11.673964	721.045752	11.848653
11.544006	713.285689	11.853671
11.188972	713.794708	11.858688
11.734215	716.681632	11.863706
11.599190	705.432233	11.868723
11.378444	715.271693	11.873741
11.719603	707.384083	11.878759
11.287261	717.989769	11.883776
11.410097	717.549511	11.888794
11.496748	713.073883	11.893811
11.566755	702.070767	11.898829
11.433226	712.322796	11.903847
11.006701	720.336583	11.908864
11.461968	721.727249	11.913882
11.564874	748.613428	11.918899
11.349353	738.412937	11.923917
11.670010	740.371711	11.928935
12.026494	748.348127	11.933952
11.943125	741.462663	11.938970
11.942909	745.614805	11.943987
11.975607	746.316591	11.949005
12.108987	736.282713	11.954023
11.868919	736.952916	11.959040
11.792813	717.147664	11.964058
11.508645	717.000411	11.969075
11.377947	746.253680	11.974093
11.581266	739.999157	11.979111
11.755538	744.895250	11.984128
11.574861	741.401900	11.989146
11.816664	740.645877	11.994163
11.727973	733.370229	11.999181
11.678321	733.621932	12.004199
11.896542	739.085750	12.009216
11.823019	738.020389	12.014234
11.875002	745.713525	12.019251
11.631405	745.987635	12.024269
11.894700	735.321381	12.029287
11.422638	747.882591	12.034304
11.700586	747.236419	12.039322
12.306998	755.231367	12.044339
12.132231	751.875103	12.049357
12.141304	740.196824	12.054375
12.108447	752.648751	12.059392
12.180325	734.984852	12.064410
12.356967	741.554053	12.069427
11.761443	753.104271	12.074445
12.248044	744.987823	12.079463
12.185989	746.166401	12.084480
12.163510	742.734981	12.089498
12.199380	733.207087	12.094515
11.821108	745.313903	12.099533
12.380313	740.769228	12.104551
12.279421	745.439191	12.109568
12.412201	738.387916	12.114586
12.522331	735.027381	12.119603
12.178136	746.388944	12.124621
12.422995	730.794786	12.129639
12.101689	731.562551	12.134656
11.810547	722.998569	12.139674
12.076986	726.870858	12.144691
12.084108	739.365470	12.149709
12.648986	742.337918	12.154727
12.452624	739.477355	12.159744
11.868771	715.317980	12.164762
12.119192	725.114124	12.169779
12.219207	733.092469	12.174797
12.304554	733.941331	12.179815
12.291730	748.263506	12.184832
12.046982	744.697884	12.189850
12.648468	732.561938	12.194867
12.301267	736.991751	12.199885
12.378120	736.993556	12.204903
11.994715	736.776891	12.209920
12.159923	731.160046	12.214938
12.157641	737.485735	12.219955
11.800475	741.062633	12.224973
12.262653	731.187670	12.229991
11.974503	740.263530	12.235008
11.890033	746.372435	12.240026
12.064008	731.777893	12.245043
12.193152	760.385806	12.250061
11.975082	771.912631	12.255079
12.026004	774.671846	12.260096
12.577355	762.885534	12.265114
12.603047	769.258572	12.270131
12.242486	776.861759	12.275149
12.647454	768.326882	12.280167
12.403310	776.767658	12.285184
12.584984	776.511832	12.290202
12.484803	771.808350	12.295219
12.269902	776.618400	12.300237
12.657182	765.053750	12.305255
12.661055	772.102020	12.310272
12.384407	774.277889	12.315290
12.489011	765.252496	12.320307
12.477565	762.650785	12.325325
12.956025	763.043224	12.330343
12.796236	766.184241	12.335360
12.645444	761.435199	12.340378
12.658524	767.455072	12.345395
12.755128	768.158206	12.350413
12.767731	763.255217	12.355431
12.747479	777.825056	12.360448
12.689501	771.549736	12.365466
12.654376	757.927147	12.370483
12.463906	777.564026	12.375501
12.655730	775.168440	12.380519
12.580244	774.364179	12.385536
12.574667	770.687683	12.390554
12.743071	763.419033	12.395571
12.348867	775.098272	12.400589
12.564343	769.089811	12.405607
12.743366	777.476697	12.410624
12.992782	787.841149	12.415642
13.425258	779.264523	12.420659
12.728342	780.607257	12.425677
12.979496	772.226021	12.430695
12.878008	768.546382	12.435712
12.301207	778.046470	12.440730
12.840154	783.778993	12.445747
12.735070	779.964834	12.450765
13.169198	792.173610	12.455783
12.934321	784.178829	12.460800
13.003474	782.767605	12.465818
13.063198	773.148162	12.470835
12.928262	775.959249	12.475853
12.924376	775.942120	12.480871
12.702712	770.101254	12.485888
13.321420	787.706063	12.490906
13.144493	783.951896	12.495923
12.663069	776.874568	12.500941
13.030717	780.699640	12.505959
13.206182	787.139452	12.510976
12.992506	788.018839	12.515994
13.279796	780.240863	12.521011
13.092701	782.799202	12.526029
13.109993	765.687493	12.531047
13.071504	767.689581	12.536064
13.005141	767.259234	12.541082
13.044424	762.131898	12.546099
12.924312	774.227466	12.551117
13.040480	785.168655	12.556135
13.231412	788.912618	12.561152
13.074742	790.835734	12.566170
13.568289	792.618038	12.571187
13.407482	783.740806	12.576205
13.122085	782.261622	12.581223
13.410739	795.547000	12.586240
13.170050	787.584471	12.591258
13.023410	769.365416	12.596275
13.094275	783.226337	12.601293
13.219298	782.823407	12.606311
13.215878	797.094574	12.611328
13.219227	801.427702	12.616346
13.427114	790.488926	12.621363
13.368135	795.620689	12.626381
12.981193	793.582704	12.631399
13.423021	788.224792	12.636416
13.551181	792.641899	12.641434
13.736463	789.472143	12.646451
13.626140	794.073614	12.651469
13.565136	797.806368	12.656487
13.147794	784.401023	12.661504
12.895434	791.728412	12.666522
13.419942	797.008294	12.671539
13.621729	798.024694	12.676557
13.579749	790.640433	12.681575
13.549167	793.263542	12.686592
13.935069	798.148002	12.691610
13.490568	796.538445	12.696627
13.287667	798.479337	12.701645
13.222077	788.901554	12.706663
13.661249	791.078894	12.711680
13.226835	791.893990	12.716698
13.638979	779.029990	12.721715
13.538971	794.642852	12.726733
13.282428	795.067893	12.731751
13.474045	790.275345	12.736768
13.305405	791.831217	12.741786
13.616365	785.039595	12.746803
13.766997	788.587893	12.751821
13.334428	787.246197	12.756839
13.458258	801.413481	12.761856
13.560713	792.934388	12.766874
13.690479	802.893998	12.771891
13.766716	815.473590	12.776909
13.678762	817.129200	12.781927
14.070451	811.332012	12.786944
13.693664	795.020592	12.791962
13.872485	790.954335	12.796979
13.527716	784.995053	12.801997
13.764465	808.013580	12.807015
13.661276	802.443031	12.812032
13.656350	812.455018	12.817050
14.142282	818.280551	12.822067
14.042962	818.172913	12.827085
14.242727	813.799899	12.832103
14.023294	783.838050	12.837120
13.693103	781.953059	12.842138
13.653132	786.678014	12.847155
13.560547	786.895088	12.852173
14.045841	808.363967	12.857191
14.523439	811.503874	12.862208
14.117735	797.690469	12.867226
14.295887	789.373541	12.872243
14.176711	777.237186	12.877261
13.704292	773.741361	12.882279
14.089920	774.255125	12.887296
14.149966	776.272716	12.892314
13.713527	781.430736	12.897331
13.678649	794.392877	12.902349
13.608816	785.979654	12.907367
13.944363	800.000947	12.912384
13.712439	816.244474	12.917402
14.095568	811.292933	12.922419
14.128300	814.176596	12.927437
13.872348	813.865062	12.932455
14.101494	823.676987	12.937472
14.097406	826.995890	12.942490
13.910247	815.771262	12.947507
14.127219	814.359226	12.952525
13.916622	820.780386	12.957543
14.364184	821.253903	12.962560
13.950327	822.346457	12.967578
13.850775	815.252355	12.972595
14.164741	817.147689	12.977613
14.110550	819.012444	12.982631
14.422110	831.093601	12.987648
14.267954	842.447545	12.992666
14.594887	838.733797	12.997683
14.404616	818.505827	13.002701
13.755382	815.074835	13.007719
14.163103	820.559226	13.012736
14.285694	835.009665	13.017754
14.338443	851.593812	13.022771
14.535521	842.198432	13.027789
14.702450	840.199005	13.032807
14.700667	835.558165	13.037824
14.409751	826.485421	13.042842
14.579302	831.361263	13.047859
14.273631	819.919548	13.052877
14.399397	834.185146	13.057895
14.847865	835.681357	13.062912
14.471434	824.411736	13.067930
14.293986	819.210866	13.072947
14.256740	829.379653	13.077965
14.588934	835.561739	13.082983
14.908743	847.429774	13.088000
14.883133	842.838432	13.093018
14.763360	826.821845	13.098035
14.366119	809.755662	13.103053
14.454699	821.661100	13.108071
14.520323	819.375126	13.113088
14.459830	830.627576	13.118106
14.596426	830.879009	13.123123
14.731514	836.763906	13.128141
14.499468	837.716593	13.133159
14.578233	832.270069	13.138176
14.563534	844.009457	13.143194
14.461410	837.142795	13.148211
14.586740	842.179758	13.153229
14.610295	840.465098	13.158247
14.822187	834.306937	13.163264
14.763800	838.860967	13.168282
14.682367	847.862875	13.173299
14.706989	834.162247	13.178317
14.500802	833.900549	13.183335
14.796036	827.967353	13.188352
14.620032	841.156557	13.193370
14.860969	844.112984	13.198387
14.873362	836.019844	13.203405
14.352336	835.659021	13.208423
15.050208	852.809861	13.213440
14.942447	860.067726	13.218458
14.878052	855.377789	13.223475
15.221590	860.167320	13.228493
15.178875	844.643006	13.233511
15.102977	825.478999	13.238528
15.106715	822.681989	13.243546
14.989452	834.446781	13.248563
15.297265	823.973368	13.253581
14.867442	827.716496	13.258599
15.329202	823.113013	13.263616
15.141593	830.116196	13.268634
15.048655	829.112688	13.273651
15.254871	823.100619	13.278669
14.945939	828.084168	13.283687
15.353358	827.330295	13.288704
15.379833	825.018905	13.293722
15.154896	831.311165	13.298739
15.231183	822.282151	13.303757
14.716078	832.887520	13.308775
15.294319	834.449671	13.313792
15.452166	834.247281	13.318810
15.255366	825.505181	13.323827
15.326912	828.922589	13.328845
15.178995	829.704610	13.333863
15.554477	822.943935	13.338880
15.370128	826.284557	13.343898
15.148185	828.837936	13.348915
14.941967	820.007255	13.353933
15.060568	830.933707	13.358951
14.874302	826.330934	13.363968
15.120225	832.420307	13.368986
15.026877	851.341261	13.374003
15.499226	857.013965	13.379021
15.628643	858.412930	13.384039
15.715648	862.814717	13.389056
15.679882	836.921273	13.394074
15.409815	831.352409	13.399091
15.395955	817.572146	13.404109
15.639018	814.915575	13.409127
15.355214	820.430007	13.414144
15.661677	820.456653	13.419162
15.496506	827.600489	13.424179
15.408162	821.389703	13.429197
15.424152	831.296493	13.434215
15.781906	840.390258	13.439232
15.586040	840.280959	13.444250
15.655085	834.407773	13.449267
15.512875	817.769133	13.454285
15.118235	827.706384	13.459303
15.744163	838.692187	13.464320
15.696907	853.498309	13.469338
15.730274	850.634992	13.474355
16.113872	847.692247	13.479373
15.810908	843.948659	13.484391
15.591875	830.766557	13.489408
16.023671	832.481526	13.494426
15.657720	825.111128	13.499443
15.666476	814.871654	13.504461
15.568989	829.852953	13.509479
15.447601	829.362123	13.514496
15.973858	835.831865	13.519514
15.839336	851.731244	13.524531
15.967071	848.818578	13.529549
15.739532	853.948301	13.534567
15.873357	857.121607	13.539584
16.003529	847.487031	13.544602
16.030279	846.513242	13.549619
16.122447	833.681802	13.554637
15.814857	830.407399	13.559655
15.872445	820.358044	13.564672
16.375770	811.963454	13.569690
15.734701	821.513749	13.574707
15.950246	811.897758	13.579725
15.559418	818.291920	13.584743
15.730932	836.465870	13.589760
16.187099	847.516635	13.594778
16.245648	857.547094	13.599795
16.307174	856.207485	13.604813
16.217117	853.708300	13.609831
16.250950	849.183202	13.614848
16.043379	824.535270	13.619866
15.864439	821.911139	13.624883
15.979387	842.041721	13.629901
16.147279	865.385632	13.634919
16.217992	849.008174	13.639936
16.429397	849.334532	13.644954
16.228813	862.116868	13.649971
16.364363	848.481345	13.654989
16.451957	853.267312	13.660007
16.326463	840.332491	13.665024
16.074692	825.226237	13.670042
16.165800	834.579574	13.675059
16.202145	843.635625	13.680077
15.978216	858.927557	13.685095
15.981675	856.074299	13.690112
16.382668	853.895073	13.695130
16.523039	864.538869	13.700147
16.385829	856.754543	13.705165
16.525487	862.736019	13.710183
16.168859	854.957250	13.715200
16.433491	845.943743	13.720218
16.184455	852.694438	13.725235
16.226858	859.431023	13.730253
16.374205	856.953323	13.735271
16.558791	860.267427	13.740288
16.528825	849.036480	13.745306
15.904453	862.958633	13.750323
16.486898	847.628197	13.755341
16.305893	847.174970	13.760359
16.367973	860.309790	13.765376
16.757328	866.671286	13.770394
16.498691	859.254993	13.775411
16.625499	865.405985	13.780429
16.857533	859.840341	13.785447
16.562930	859.220684	13.790464
16.785719	845.489363	13.795482
16.373724	856.195207	13.800499
16.638429	868.606027	13.805517
16.734070	872.845493	13.810535
16.705821	886.929346	13.815552
17.108200	879.460982	13.820570
16.711540	870.278839	13.825587
16.467892	852.116457	13.830605
16.794552	858.395808	13.835623
16.517593	874.911652	13.840640
16.963493	880.943987	13.845658
16.760752	890.612011	13.850675
16.735655	884.127016	13.855693
16.799320	884.012026	13.860711
17.109675	881.337730	13.865728
17.070228	884.150770	13.870746
16.856527	892.080665	13.875763
16.854340	876.087206	13.880781
17.140863	878.253767	13.885799
16.973850	887.866780	13.890816
16.943380	878.355860	13.895834
16.915947	887.055909	13.900851
17.052394	878.760979	13.905869
17.102360	878.346734	13.910887
17.094025	887.620195	13.915904
17.231802	879.225064	13.920922
17.047184	880.417706	13.925939
16.861919	881.633285	13.930957
16.972114	881.368703	13.935975
16.675166	886.693732	13.940992
16.650865	873.420172	13.946010
16.817907	885.290060	13.951027
16.700426	879.995515	13.956045
17.045956	883.525700	13.961063
16.915409	909.514098	13.966080
17.285396	910.924682	13.971098
17.289185	915.070008	13.976115
17.472398	910.575019	13.981133
17.652335	898.602782	13.986151
17.645858	898.042182	13.991168
17.509625	878.725608	13.996186
17.289482	875.197319	14.001203
17.402368	874.685782	14.006221
17.423766	865.230952	14.011239
17.108711	868.160092	14.016256
17.143305	871.255034	14.021274
16.954831	882.436758	14.026291
17.298739	896.082711	14.031309
17.949065	895.637942	14.036327
17.561541	913.609833	14.041344
17.746891	885.298893	14.046362
17.549537	891.270534	14.051379
17.302531	876.917243	14.056397
17.709480	874.490914	14.061415
17.255070	878.789691	14.066432
17.567948	878.672587	14.071450
17.472210	902.009636	14.076467
17.762053	899.467936	14.081485
17.766552	892.326982	14.086503
17.615403	911.722439	14.091520
17.809871	889.537335	14.096538
17.795024	879.485937	14.101555
17.806955	876.559634	14.106573
17.861109	872.191476	14.111591
17.724154	878.694076	14.116608
17.701179	872.344242	14.121626
17.428406	872.624553	14.126643
17.323775	886.783025	14.131661
17.514363	884.514868	14.136679
17.581128	901.717703	14.141696
18.072306	895.943602	14.146714
17.715269	895.637552	14.151731
17.538999	898.856896	14.156749
17.972779	905.550081	14.161767
17.634429	905.806491	14.166784
17.865300	905.993437	14.171802
17.542584	902.502562	14.176819
17.456182	909.140791	14.181837
18.026175	897.849139	14.186855
17.637004	903.638250	14.191872
17.551779	901.634823	14.196890
18.017273	917.704654	14.201907
17.986949	928.870118	14.206925
18.215379	926.535181	14.211943
18.173413	930.295229	14.216960
18.143327	927.539807	14.221978
18.355901	931.362891	14.226995
17.963104	913.771343	14.232013
18.014744	926.772734	14.237031
18.140055	936.149708	14.242048
18.522727	920.738354	14.247066
18.187831	922.458696	14.252083
17.841665	915.414158	14.257101
18.212537	905.596488	14.262119
18.160630	928.405364	14.267136
18.189227	928.462971	14.272154
18.543962	931.770426	14.277171
18.338594	931.538703	14.282189
18.538605	915.632633	14.287207
18.322075	930.238005	14.292224
18.291642	923.382485	14.297242
18.673303	924.975950	14.302259
18.240585	925.118352	14.307277
18.545657	904.767178	14.312295
17.944683	904.285139	14.317312
18.237967	923.808903	14.322330
18.713949	922.076840	14.327347
18.615826	934.190649	14.332365
18.677645	915.657984	14.337383
18.572641	933.889850	14.342400
18.881590	916.279363	14.347418
19.097359	902.660747	14.352435
18.492484	907.767327	14.357453
18.616779	899.381596	14.362471
18.635456	891.657597	14.367488
18.332637	893.430794	14.372506
18.438385	894.482458	14.377523
18.199279	902.295909	14.382541
18.559349	904.859007	14.387559
18.391899	929.329697	14.392576
18.454739	918.980446	14.397594
18.635095	920.890395	14.402611
18.401929	926.722915	14.407629
18.870045	920.160237	14.412647
18.524940	929.211473	14.417664
18.669538	928.030639	14.422682
18.962353	929.283634	14.427699
18.706329	933.377527	14.432717
18.776967	924.294181	14.437735
18.964032	928.961291	14.442752
18.768628	921.766661	14.447770
18.890508	916.401648	14.452787
18.421093	920.458177	14.457805
18.847130	920.221799	14.462823
18.993263	928.999568	14.467840
18.967805	934.864683	14.472858
19.096332	934.105721	14.477875
19.029680	928.367601	14.482893
19.053396	923.218870	14.487911
19.044460	932.128055	14.492928
18.714523	922.504222	14.497946
19.291954	931.215934	14.502963
19.319252	947.280172	14.507981
19.037383	934.538505	14.512999
19.279179	929.981575	14.518016
19.143456	927.915538	14.523034
18.909163	923.011475	14.528051
19.162002	941.283803	14.533069
19.248198	937.342637	14.538087
19.363539	951.937765	14.543104
19.201838	945.841888	14.548122
19.698296	934.944676	14.553139
19.142287	932.051794	14.558157
19.348016	916.415498	14.563175
19.304331	918.631811	14.568192
19.003421	925.009387	14.573210
19.216436	927.686538	14.578227
19.326363	943.305501	14.583245
19.631744	947.214810	14.588263
19.633947	953.444784	14.593280
19.280760	950.492599	14.598298
19.460557	937.298523	14.603315
19.613593	953.483105	14.608333
19.388357	956.710553	14.613351
19.506138	954.685971	14.618368
19.445943	959.424555	14.623386
19.705306	952.339176	14.628403
19.461991	949.139347	14.633421
19.691449	961.201995	14.638439
19.968878	941.101655	14.643456
19.700363	940.031404	14.648474
19.419156	932.028161	14.653491
19.539042	942.766719	14.658509
19.541290	948.129810	14.663527
19.420299	952.139692	14.668544
19.662663	954.059867	14.673562
19.856031	950.454271	14.678579
19.907784	955.468791	14.683597
19.853587	949.682648	14.688615
19.957601	959.105077	14.693632
19.377606	956.340246	14.698650
19.595522	965.472447	14.703667
19.618091	958.392442	14.708685
19.915201	952.661216	14.713703
19.858866	956.494498	14.718720
19.408723	956.233650	14.723738
20.129762	948.523946	14.728755
19.507941	957.445465	14.733773
19.569060	949.703992	14.738791
19.721572	962.695436	14.743808
19.773805	984.211130	14.748826
19.966277	975.582931	14.753843
20.211400	979.066553	14.758861
20.282877	984.346575	14.763879
20.396276	980.667688	14.768896
20.272472	979.525299	14.773914
20.175526	982.356420	14.778931
20.353383	982.631249	14.783949
20.247234	977.392267	14.788967
20.284070	961.138870	14.793984
19.773020	953.296215	14.799002
20.118182	970.315251	14.804019
20.252196	976.399262	14.809037
20.281076	980.494405	14.814055
20.442437	978.803995	14.819072
20.334391	985.053186	14.824090
20.330117	971.265494	14.829107
20.260508	974.632257	14.834125
20.481013	977.928839	14.839143
20.548665	972.732878	14.844160
20.347201	978.226674	14.849178
20.421745	973.276282	14.854195
20.548423	964.950347	14.859213
20.248819	967.911100	14.864231
20.548078	962.753725	14.869248
20.217309	963.959110	14.874266
20.618464	968.566645	14.879283
20.169308	968.242456	14.884301
20.453465	968.738455	14.889319
20.755276	971.997784	14.894336
20.338330	971.844521	14.899354
20.461399	975.369765	14.904371
20.389341	985.159043	14.909389
20.310604	970.291426	14.914407
20.438109	975.229469	14.919424
20.472838	974.451759	14.924442
20.811831	972.264952	14.929459
20.674678	979.384547	14.934477
20.626431	965.858216	14.939495
20.945133	960.276738	14.944512
20.319829	983.883675	14.949530
20.770040	982.920988	14.954547
20.847591	995.908412	14.959565
20.795564	992.736894	14.964583
21.133179	998.700767	14.969600
21.443861	1003.357116	14.974618
20.874902	986.735575	14.979635
21.123260	972.399726	14.984653
21.019964	969.535943	14.989671
20.717439	970.221003	14.994688
20.819904	966.836295	14.999706
20.864977	984.205869	15.004723
21.197174	989.126525	15.009741
21.146101	994.878496	15.014759
21.248859	991.368854	15.019776
21.254174	978.526552	15.024794
20.917972	961.160006	15.029811
20.903399	986.107894	15.034829
21.083916	981.555959	15.039847
21.025732	989.467486	15.044864
20.949523	1002.515851	15.049882
21.301815	982.571955	15.054899
21.063990	994.820196	15.059917
21.047291	996.986204	15.064935
21.224478	980.092377	15.069952
21.321652	995.412667	15.074970
21.271229	992.203292	15.079987
21.243238	994.727500	15.085005
21.409929	1001.712854	15.090023
21.421338	988.410659	15.095040
21.029646	989.714484	15.100058
21.521068	984.062435	15.105075
21.256698	985.001381	15.110093
21.662504	992.936512	15.115111
21.693679	985.260688	15.120128
21.740973	995.435887	15.125146
21.552088	986.336149	15.130163
21.816922	982.610979	15.135181
21.685270	1004.205900	15.140199
21.774061	984.051554	15.145216
21.229035	992.265741	15.150234
21.565110	998.331426	15.155251
21.822066	986.283313	15.160269
21.628197	996.857359	15.165287
21.884217	985.270935	15.170304
21.492513	991.695033	15.175322
21.816025	998.609399	15.180339
22.002565	976.638434	15.185357
21.503625	997.181145	15.190375
21.587234	987.430280	15.195392
21.735436	985.577801	15.200410
21.607578	984.993466	15.205427
21.603355	997.929260	15.210445
21.895749	1016.097618	15.215463
22.425468	1006.664292	15.220480
21.782849	1003.853117	15.225498
22.023043	992.315556	15.230515
21.946207	981.746277	15.235533
21.750615	994.133380	15.240551
22.351429	1006.356114	15.245568
22.033324	1001.608962	15.250586
21.722473	1005.652201	15.255603
22.269716	1013.854963	15.260621
22.156354	1015.236002	15.265639
22.327491	1018.675767	15.270656
21.916989	1010.987893	15.275674
22.289377	1022.496550	15.280691
22.370026	1008.935202	15.285709
22.431522	1017.374509	15.290727
22.162330	1002.327642	15.295744
22.281373	997.436610	15.300762
22.229578	998.219288	15.305779
22.457572	997.192748	15.310797
22.009639	996.443135	15.315815
22.339459	1008.956674	15.320832
22.400912	1010.282943	15.325850
22.651484	1007.591147	15.330867
22.612667	1011.043169	15.335885
22.378775	993.879128	15.340903
22.050977	999.511997	15.345920
22.590681	1010.044439	15.350938
22.274067	1004.793090	15.355955
22.135146	1012.993909	15.360973
22.096085	1024.792470	15.365991
22.201379	1007.710627	15.371008
22.251522	1015.484700	15.376026
22.229494	1009.931858	15.381043
22.336550	1012.354436	15.386061
22.373140	1038.111825	15.391079
23.110393	1033.770182	15.396096
22.808714	1040.664281	15.401114
22.663802	1041.828724	15.406131
23.006198	1034.972064	15.411149
22.749984	1044.130507	15.416167
22.985029	1031.302845	15.421184
22.804436	1021.441905	15.426202
22.784872	1024.757602	15.431219
23.188276	1022.776445	15.436237
22.811242	1018.136647	15.441255
22.790702	1003.150147	15.446272
22.721319	1017.341097	15.451290
22.934085	1032.527185	15.456307
23.182937	1032.440932	15.461325
23.083208	1043.634580	15.466343
23.142592	1032.939919	15.471360
23.265481	1023.978368	15.476378
23.274303	1010.925554	15.481395
23.349422	999.045154	15.486413
22.877769	1008.069817	15.491431
22.826045	995.183983	15.496448
22.800594	998.167339	15.501466
22.931828	1024.897182	15.506483
23.071491	1027.530675	15.511501
22.915509	1034.300318	15.516519
23.173630	1038.197876	15.521536
23.228163	1035.651641	15.526554
23.082672	1036.098782	15.531571
23.512894	1043.257891	15.536589
23.205249	1038.451824	15.541607
23.427175	1038.324359	15.546624
23.287898	1033.980937	15.551642
23.293663	1028.273619	15.556659
23.490863	1030.034564	15.561677
23.363286	1041.944896	15.566695
23.532779	1027.298264	15.571712
23.609221	1037.980004	15.576730
23.355759	1035.310287	15.581747
23.461574	1021.906158	15.586765
23.678765	1039.164393	15.591783
23.398241	1024.373271	15.596800
23.503589	1033.532775	15.601818
23.175368	1041.078591	15.606835
23.365858	1033.544595	15.611853
23.296761	1044.270268	15.616871
23.403890	1054.400388	15.621888
23.745413	1063.544106	15.626906
23.776446	1060.390830	15.631923
24.471881	1045.557088	15.636941
24.334519	1044.852098	15.641959
24.195007	1033.844496	15.646976
24.339018	1025.583271	15.651994
24.006419	1019.500154	15.657011
24.209281	1017.947838	15.662029
23.920134	1019.252925	15.667047
24.231336	1026.478832	15.672064
23.956377	1024.473579	15.677082
23.989440	1015.053239	15.682099
24.180250	1006.396857	15.687117
23.585915	1021.032372	15.692135
23.538406	1009.896709	15.697152
24.046553	1013.850663	15.702170
24.087874	1026.059296	15.707187
23.912959	1016.048234	15.712205
24.149257	1026.212394	15.717223
24.047768	1019.012925	15.722240
24.162385	1011.416785	15.727258
23.938070	1023.610563	15.732275
24.131406	1019.103242	15.737293
23.956581	1025.546819	15.742311
23.838713	1038.538626	15.747328
24.465439	1036.238721	15.752346
24.015546	1050.097471	15.757363
24.609822	1048.467775	15.762381
24.251354	1043.452031	15.767399
24.632509	1051.256152	15.772416
24.696863	1038.616507	15.777434
24.452509	1047.191005	15.782451
24.477824	1047.595552	15.787469
24.517397	1048.413617	15.792487
24.379634	1062.834671	15.797504
24.729724	1053.576350	15.802522
24.347276	1047.882006	15.807539
24.673470	1048.506865	15.812557
24.397055	1053.970856	15.817575
24.302031	1051.812264	15.822592
24.612640	1049.409504	15.827610
24.192653	1049.384181	15.832627
24.703077	1051.645833	15.837645
24.728030	1046.378176	15.842663
24.464638	1041.682097	15.847680
24.641448	1054.238672	15.852698
24.313709	1053.392336	15.857715
24.743526	1060.373401	15.862733
24.862162	1069.980852	15.867751
24.690033	1075.848412	15.872768
24.945014	1079.880533	15.877786
24.834027	1083.562768	15.882803
25.055052	1076.986338	15.887821
24.975668	1083.036573	15.892839
25.124256	1082.997199	15.897856
25.040070	1076.702074	15.902874
24.433456	1079.305776	15.907891
25.027270	1071.200472	15.912909
24.891220	1083.821762	15.917927
24.985433	1077.629220	15.922944
25.284925	1071.971165	15.927962
24.893989	1067.808667	15.932979
25.097008	1077.348054	15.937997
25.391274	1076.896285	15.943015
25.160599	1080.377469	15.948032
25.348855	1064.105140	15.953050
25.169504	1081.075173	15.958067
25.163659	1068.549449	15.963085
25.143205	1069.863968	15.968103
25.054846	1082.334290	15.973120
25.592338	1074.057810	15.978138
25.275247	1072.870793	15.983155
25.158432	1081.553149	15.988173
25.705143	1088.345450	15.993191
25.760482	1089.843082	15.998208
25.889368	1084.879246	16.003226
25.294797	1072.901912	16.008243
25.334679	1064.636420	16.013261
25.668969	1069.589527	16.018279
25.494653	1074.941000	16.023296
25.732859	1071.050258	16.028314
25.675726	1085.982134	16.033331
25.617366	1082.671410	16.038349
26.027104	1081.950405	16.043367
25.723284	1084.583585	16.048384
25.776410	1068.855148	16.053402
25.610537	1068.752601	16.058419
25.764031	1086.486790	16.063437
25.704811	1084.001464	16.068455
25.500388	1098.755758	16.073472
25.975080	1084.330639	16.078490
25.712275	1095.492031	16.083507
25.708047	1087.695551	16.088525
26.017047	1084.384936	16.093543
25.787817	1096.524081	16.098560
26.116928	1094.647894	16.103578
25.863623	1089.181167	16.108595
26.071751	1080.771348	16.113613
26.218133	1089.979017	16.118631
26.069012	1089.220465	16.123648
26.379669	1093.450834	16.128666
26.112727	1099.711961	16.133683
26.342923	1093.282016	16.138701
26.454861	1090.544623	16.143719
26.263286	1089.500813	16.148736
26.463510	1084.452169	16.153754
26.038029	1095.613874	16.158771
26.260105	1081.545018	16.163789
26.659674	1091.768545	16.168807
26.076792	1095.897403	16.173824
26.390113	1083.327584	16.178842
26.093150	1089.291357	16.183859
26.001625	1089.327877	16.188877
26.641630	1083.032739	16.193895
26.333640	1082.251040	16.198912
26.340926	1080.301286	16.203930
26.172912	1088.227077	16.208947
26.573961	1104.662715	16.213965
26.822358	1114.367825	16.218983
26.667994	1120.435780	16.224000
26.748689	1120.528669	16.229018
26.785626	1121.831542	16.234035
26.552403	1112.258230	16.239053
27.080700	1121.910596	16.244071
26.555850	1113.249703	16.249088
26.837204	1107.478707	16.254106
27.060414	1122.004704	16.259123
27.066379	1105.783514	16.264141
26.949179	1089.362849	16.269159
26.703495	1092.449732	16.274176
26.836840	1088.865439	16.279194
26.872934	1092.881972	16.284211
26.685714	1105.818378	16.289229
26.680318	1119.414398	16.294247
27.139355	1113.876789	16.299264
27.114457	1099.430098	16.304282
27.064943	1115.898873	16.309299
26.906090	1109.464523	16.314317
27.179403	1115.719436	16.319335
26.992731	1121.123943	16.324352
27.055098	1106.389838	16.329370
27.031641	1113.689886	16.334387
26.930622	1111.839508	16.339405
27.092384	1114.653783	16.344423
27.016341	1118.353869	16.349440
27.308633	1105.263578	16.354458
27.163411	1114.071690	16.359475
27.415152	1124.135446	16.364493
27.646492	1126.503652	16.369511
27.469681	1130.845684	16.374528
27.464202	1110.747098	16.379546
27.786451	1105.872344	16.384563
27.329315	1105.646501	16.389581
27.548462	1100.803548	16.394599
27.333604	1106.956482	16.399616
27.709072	1120.835767	16.404634
27.972864	1119.182934	16.409651
27.590260	1118.498981	16.414669
27.772499	1105.604997	16.419687
27.346876	1103.099718	16.424704
27.538514	1113.933313	16.429722
27.813677	1114.034412	16.434739
27.673434	1126.625531	16.439757
27.808347	1120.347912	16.444775
27.887899	1134.456789	16.449792
27.998721	1128.944833	16.454810
28.248922	1122.678275	16.459827
28.040949	1117.123154	16.464845
28.215051	1118.791486	16.469863
27.821337	1119.466428	16.474880
28.214797	1113.425174	16.479898
28.077101	1108.434923	16.484915
27.837589	1109.507147	16.489933
28.102054	1111.460889	16.494951
28.144186	1116.539049	16.499968
27.981455	1111.192955	16.504986
28.228388	1110.995030	16.510003
28.061637	1128.491686	16.515021
28.309864	1115.323840	16.520039
28.227610	1127.796142	16.525056
28.236782	1128.251777	16.530074
28.226075	1113.042617	16.535091
27.985015	1120.606936	16.540109
28.402151	1119.214542	16.545127
27.993892	1120.709470	16.550144
28.081157	1116.909003	16.555162
28.224309	1115.538464	16.560179
27.850649	1128.583442	16.565197
28.488116	1118.326962	16.570215
28.117418	1117.150769	16.575232
28.342935	1139.669962	16.580250
28.548984	1139.039299	16.585267
28.428447	1148.732181	16.590285
28.921536	1153.827550	16.595303
28.813908	1146.992263	16.600320
28.599639	1146.985691	16.605338
28.584229	1154.058284	16.610355
28.611805	1146.252582	16.615373
28.728640	1140.087767	16.620391
28.431242	1154.839174	16.625408
28.656528	1146.121415	16.630426
28.890628	1140.640256	16.635443
28.743878	1152.239326	16.640461
29.101283	1145.790700	16.645479
28.935002	1152.363507	16.650496
28.796140	1151.692612	16.655514
29.379526	1140.425142	16.660531
28.870291	1153.083163	16.665549
28.922536	1141.242745	16.670567
29.072280	1136.745644	16.675584
28.938016	1130.542813	16.680602
29.323869	1139.222633	16.685619
29.159696	1146.588463	16.690637
29.207205	1158.676414	16.695655
29.116157	1140.598493	16.700672
29.201584	1140.860650	16.705690
29.107054	1144.172721	16.710707
28.846885	1145.271389	16.715725
29.392106	1159.443273	16.720743
29.504014	1170.634516	16.725760
29.595473	1177.551490	16.730778
29.914809	1164.334849	16.735795
29.374472	1155.673341	16.740813
29.285732	1136.012822	16.745831
29.326368	1145.751497	16.750848
29.315610	1165.875724	16.755866
29.873802	1165.822197	16.760883
29.762912	1176.212012	16.765901
29.767918	1156.658788	16.770919
29.958430	1157.396217	16.775936
29.741759	1147.785704	16.780954
29.699923	1127.253609	16.785971
29.486365	1134.943881	16.790989
29.332786	1147.636810	16.796007
29.706755	1155.816718	16.801024
29.896566	1164.796819	16.806042
29.870175	1164.576158	16.811059
29.742515	1161.926567	16.816077
29.597168	1161.507883	16.821095
30.050736	1162.675190	16.826112
29.676574	1164.190270	16.831130
30.108861	1161.066713	16.836147
30.083874	1169.407226	16.841165
30.232170	1156.575491	16.846183
30.042499	1169.869778	16.851200
29.723992	1165.550623	16.856218
29.807324	1159.256516	16.861235
29.599486	1180.134668	16.866253
30.245175	1183.115206	16.871271
30.597621	1187.057639	16.876288
30.247439	1189.568794	16.881306
30.422863	1188.598560	16.886323
30.279862	1191.486240	16.891341
30.333874	1193.561370	16.896359
30.493921	1198.181953	16.901376
30.855806	1203.617079	16.906394
30.606005	1175.761016	16.911411
30.612506	1162.716132	16.916429
30.494271	1157.113890	16.921447
30.663344	1156.674542	16.926464
30.219088	1160.373292	16.931482
30.251685	1148.151532	16.936499
30.316118	1176.554514	16.941517
30.155644	1172.891217	16.946535
30.354278	1186.211493	16.951552
30.426730	1186.351997	16.956570
30.843620	1184.543957	16.961587
30.656073	1186.642472	16.966605
30.426088	1187.152784	16.971623
30.490712	1186.869650	16.976640
30.760805	1203.275468	16.981658
30.953551	1202.704472	16.986675
31.243275	1209.948088	16.991693
31.002338	1206.629916	16.996711
31.069665	1207.995088	17.001728
30.555415	1196.495840	17.006746
31.267187	1200.661726	17.011763
31.130776	1216.695828	17.016781
30.898484	1205.384785	17.021799
31.085443	1208.955619	17.026816
31.048048	1218.547025	17.031834
31.540372	1210.773527	17.036851
31.735690	1207.264385	17.041869
31.417263	1202.021337	17.046887
31.362266	1181.966465	17.051904
31.454988	1193.990288	17.056922
31.220008	1181.806422	17.061939
31.343035	1195.776106	17.066957
31.214723	1206.396933	17.071975
31.239906	1213.704736	17.076992
31.074260	1214.207369	17.082010
31.181480	1212.401688	17.087027
31.110490	1219.132371	17.092045
31.540061	1212.471233	17.097063
31.511477	1201.852791	17.102080
30.972188	1227.651538	17.107098
31.199214	1220.131096	17.112115
31.403410	1239.224976	17.117133
31.926516	1239.216218	17.122151
32.176632	1233.086024	17.127168
31.743823	1245.439411	17.132186
32.262393	1234.755132	17.137203
32.253754	1241.140140	17.142221
31.925321	1228.242268	17.147239
32.237990	1219.388590	17.152256
32.424305	1203.517158	17.157274
32.468991	1202.014482	17.162291
32.213512	1192.650079	17.167309
32.004546	1198.800895	17.172327
32.371156	1190.539995	17.177344
32.138208	1186.442877	17.182362
32.284288	1198.348849	17.187379
32.197354	1189.989304	17.192397
31.731138	1193.771599	17.197415
32.201625	1199.782383	17.202432
32.146343	1187.656794	17.207450
32.504862	1178.573749	17.212467
31.868564	1193.729959	17.217485
31.902646	1188.191497	17.222503
32.311648	1196.746088	17.227520
32.181611	1217.478582	17.232538
32.714224	1216.628031	17.237555
32.431150	1225.461742	17.242573
32.561011	1219.505340	17.247591
32.615595	1223.905207	17.252608
32.761123	1227.874365	17.257626
32.927518	1228.623853	17.262643
32.872536	1204.876619	17.267661
32.319304	1199.626909	17.272679
32.678131	1197.575747	17.277696
32.746714	1211.715637	17.282714
32.883914	1214.741240	17.287731
32.952007	1233.612959	17.292749
32.737007	1214.445963	17.297767
33.160531	1216.793052	17.302784
32.787375	1211.509644	17.307802
32.754868	1206.674391	17.312819
32.667085	1214.277787	17.317837
32.703078	1218.608886	17.322855
33.092165	1215.540481	17.327872
32.659346	1221.525377	17.332890
32.819207	1214.784418	17.337907
32.941268	1217.456084	17.342925
32.881862	1226.894465	17.347943
32.676446	1223.837700	17.352960
33.014851	1229.755577	17.357978
33.205421	1241.101168	17.362995
33.038420	1242.057892	17.368013
33.448233	1252.099154	17.373031
33.389344	1252.298167	17.378048
33.349141	1255.135805	17.383066
33.399519	1251.231576	17.388083
33.788447	1250.960587	17.393101
33.314290	1244.750304	17.398119
33.506449	1243.796983	17.403136
33.294536	1251.061123	17.408154
33.643486	1243.078661	17.413171
33.727283	1242.145019	17.418189
33.416298	1252.104244	17.423207
33.763231	1243.189978	17.428224
33.418707	1248.286809	17.433242
33.445340	1245.900047	17.438259
33.722295	1238.992703	17.443277
33.636367	1242.030974	17.448295
34.090103	1252.370048	17.453312
33.715942	1257.220638	17.458330
33.681118	1259.566323	17.463347
34.055555	1273.912183	17.468365
33.978018	1280.667987	17.473383
34.290541	1270.606617	17.478400
34.431664	1280.772405	17.483418
34.239683	1263.418782	17.488435
34.403380	1244.327730	17.493453
33.991624	1243.760382	17.498471
34.054645	1240.642525	17.503488
33.877196	1256.312248	17.508506
34.212472	1256.604566	17.513523
34.365894	1274.621028	17.518541
34.174660	1276.555032	17.523559
34.612715	1273.324413	17.528576
34.442894	1267.704675	17.533594
34.397529	1263.525955	17.538611
34.657760	1279.407386	17.543629
34.327629	1272.266345	17.548647
34.452081	1267.647224	17.553664
34.398708	1274.326406	17.558682
34.491736	1270.095291	17.563699
34.810267	1273.586730	17.568717
34.379500	1280.124176	17.573735
34.620671	1273.672464	17.578752
34.635719	1271.609019	17.583770
34.193668	1267.484632	17.588787
34.509455	1259.656634	17.593805
34.525636	1272.468440	17.598823
34.649332	1272.025763	17.603840
34.685325	1290.715287	17.608858
34.957263	1302.741269	17.613875
35.092142	1285.196030	17.618893
35.011620	1296.474273	17.623911
35.318361	1297.249580	17.628928
35.371039	1283.000691	17.633946
35.267856	1278.039715	17.638963
35.367251	1267.034388	17.643981
35.124720	1264.687182	17.648999
35.232764	1260.679341	17.654016
34.956325	1262.165094	17.659034
34.941410	1283.962343	17.664051
35.575957	1285.507367	17.669069
34.973945	1290.178921	17.674087
35.389688	1283.424776	17.679104
35.496320	1284.109548	17.684122
35.439831	1285.456413	17.689139
35.575945	1282.793719	17.694157
35.417583	1293.312108	17.699175
35.385694	1290.411665	17.704192
35.470348	1292.648255	17.709210
35.284787	1296.675490	17.714227
35.835685	1286.643212	17.719245
35.581579	1297.364404	17.724263
35.478978	1284.821624	17.729280
35.268492	1280.985097	17.734298
35.751262	1304.136720	17.739315
36.027398	1304.061704	17.744333
35.878573	1315.286494	17.749351
35.813555	1310.092070	17.754368
36.327758	1318.487044	17.759386
36.036561	1311.061444	17.764403
36.221730	1309.056286	17.769421
36.332514	1296.751026	17.774439
35.953718	1283.248925	17.779456
36.077471	1289.901598	17.784474
35.990649	1299.876559	17.789491
36.234940	1298.753227	17.794509
36.128753	1317.326537	17.799527
36.218958	1311.472307	17.804544
36.427814	1312.825712	17.809562
35.841559	1321.856603	17.814579
36.312586	1303.773978	17.819597
35.838926	1311.956858	17.824615
36.166075	1311.646675	17.829632
36.329519	1309.693524	17.834650
36.035511	1310.834600	17.839667
36.365445	1317.633502	17.844685
36.301114	1331.820069	17.849703
36.649627	1334.878876	17.854720
37.211249	1332.055911	17.859738
36.859739	1333.208066	17.864755
37.026422	1328.741372	17.869773
36.865190	1326.377179	17.874791
36.936033	1317.153037	17.879808
36.905327	1298.579795	17.884826
36.571390	1308.844772	17.889843
37.130259	1311.309843	17.894861
36.586222	1326.409802	17.899879
36.907329	1327.438799	17.904896
37.590493	1333.508375	17.909914
37.283734	1317.431539	17.914931
37.200225	1311.695568	17.919949
36.835145	1303.733446	17.924967
36.954416	1304.574373	17.929984
37.322163	1316.782731	17.935002
37.033875	1330.153680	17.940019
37.188268	1331.704838	17.945037
37.283542	1332.849293	17.950055
37.277252	1326.739587	17.955072
37.238858	1327.632747	17.960090
37.071420	1339.297375	17.965107
37.617390	1324.774046	17.970125
37.436175	1337.847626	17.975143
37.600941	1333.733754	17.980160
37.554354	1323.587817	17.985178
37.034103	1328.810352	17.990195
37.438113	1333.140502	17.995213
37.768385	1332.729031	18.000231
37.646260	1332.214786	18.005248
37.908819	1328.304997	18.010266
37.501309	1318.418282	18.015283
37.510082	1348.038469	18.020301
37.859778	1353.298132	18.025319
38.030004	1368.352725	18.030336
38.132221	1352.596597	18.035354
38.155969	1354.103608	18.040371
38.038531	1360.685752	18.045389
37.820537	1374.443489	18.050407
38.055516	1355.683775	18.055424
38.296560	1358.685554	18.060442
38.051968	1367.751141	18.065459
38.180393	1342.598788	18.070477
38.413254	1355.925759	18.075495
38.225690	1357.877471	18.080512
38.047651	1350.503418	18.085530
38.211184	1358.948096	18.090547
38.199277	1353.053252	18.095565
38.190244	1357.321960	18.100583
38.154241	1360.494897	18.105600
38.476099	1355.126897	18.110618
38.180770	1355.551373	18.115635
38.568306	1371.443157	18.120653
38.771035	1386.870885	18.125671
38.667486	1385.014397	18.130688
38.831964	1385.167053	18.135706
38.709496	1382.298881	18.140723
38.825685	1378.079065	18.145741
38.763256	1376.300613	18.150759
39.100526	1380.766591	18.155776
39.185871	1374.140813	18.160794
39.015080	1379.076713	18.165811
39.265967	1367.965978	18.170829
39.004419	1353.899441	18.175847
38.886842	1341.866886	18.180864
39.358481	1349.353695	18.185882
39.123060	1358.241015	18.190899
39.167904	1354.748242	18.195917
39.202446	1360.481380	18.200935
39.152756	1364.767043	18.205952
39.565658	1359.780394	18.210970
39.245835	1373.383132	18.215987
39.106818	1366.391935	18.221005
39.416944	1360.453516	18.226023
39.057526	1380.123512	18.231040
39.283624	1363.494665	18.236058
39.150177	1366.571124	18.241075
39.097337	1366.536497	18.246093
39.153631	1360.852000	18.251111
38.762660	1380.466393	18.256128
39.550445	1388.212742	18.261146
39.229924	1391.385071	18.266163
39.246256	1396.311115	18.271181
39.282014	1397.968879	18.276199
39.157764	1407.533030	18.281216
39.883341	1420.351335	18.286234
40.375609	1416.530121	18.291251
40.471995	1409.609830	18.296269
40.082392	1398.747412	18.301287
40.140644	1385.948081	18.306304
40.275480	1387.938238	18.311322
39.827515	1388.444623	18.316339
40.081490	1380.792896	18.321357
40.092671	1378.525381	18.326375
40.214772	1384.016730	18.331392
40.640143	1378.170071	18.336410
40.385031	1380.993057	18.341427
40.228046	1383.355602	18.346445
40.197304	1380.632091	18.351463
40.344389	1389.908516	18.356480
40.582692	1393.719691	18.361498
40.525158	1402.550282	18.366515
40.826284	1412.168140	18.371533
40.942886	1384.508197	18.376551
40.707237	1384.166428	18.381568
40.493112	1379.293427	18.386586
40.566341	1384.165780	18.391603
40.585614	1382.242939	18.396621
40.873280	1390.076265	18.401639
40.844339	1408.075782	18.406656
41.017539	1405.546682	18.411674
40.810513	1404.594956	18.416691
40.831460	1409.388371	18.421709
40.992378	1410.152747	18.426727
40.872278	1398.907457	18.431744
41.083264	1402.467280	18.436762
41.104062	1402.541136	18.441779
41.050344	1402.399780	18.446797
41.536670	1407.107040	18.451815
41.411092	1405.120154	18.456832
41.318782	1393.569335	18.461850
41.080462	1407.804013	18.466867
41.533195	1400.868140	18.471885
41.498084	1393.753870	18.476903
40.966312	1398.544537	18.481920
41.431307	1394.249166	18.486938
41.319825	1402.812926	18.491955
40.822951	1406.901081	18.496973
41.320921	1393.804703	18.501991
41.458775	1421.856686	18.507008
41.948216	1423.920317	18.512026
42.090124	1436.098778	18.517043
41.996803	1426.718260	18.522061
42.175901	1405.682619	18.527079
41.797107	1400.294776	18.532096
41.836105	1384.919085	18.537114
41.820744	1388.723365	18.542131
41.796485	1402.500286	18.547149
42.086278	1385.416860	18.552167
41.897964	1393.764211	18.557184
42.088032	1418.170301	18.562202
42.158159	1421.999433	18.567219
42.138382	1432.975458	18.572237
42.547895	1424.678018	18.577255
42.327244	1433.357065	18.582272
42.085993	1418.845840	18.587290
41.815966	1424.798795	18.592307
41.915429	1421.513485	18.597325
42.361402	1435.194228	18.602343
42.296776	1438.497286	18.607360
42.553971	1425.652646	18.612378
42.651779	1426.471147	18.617395
42.596952	1435.668186	18.622413
42.527421	1427.097792	18.627431
42.364449	1427.998553	18.632448
42.681111	1428.439796	18.637466
42.748170	1429.738899	18.642483
42.584715	1436.318643	18.647501
42.689319	1422.373203	18.652519
42.637708	1429.090737	18.657536
42.659805	1434.215811	18.662554
42.857119	1446.208378	18.667571
42.540753	1455.681292	18.672589
43.000517	1451.978614	18.677607
42.409772	1447.993102	18.682624
43.033318	1453.964327	18.687642
42.818296	1453.954925	18.692659
42.799900	1456.136138	18.697677
43.138825	1473.264428	18.702695
43.193404	1477.836983	18.707712
43.697581	1472.579149	18.712730
43.747569	1476.129576	18.717747
43.483481	1476.751422	18.722765
43.732724	1470.693513	18.727783
43.889242	1470.629407	18.732800
43.749690	1451.680519	18.737818
43.604218	1432.127996	18.742835
43.222205	1440.866581	18.747853
43.667456	1447.030432	18.752871
43.951726	1465.441184	18.757888
44.071507	1472.856886	18.762906
43.991178	1466.924296	18.767923
43.604049	1465.065454	18.772941
43.857405	1461.391962	18.777959
43.721355	1461.706864	18.782976
43.692981	1463.530329	18.787994
43.990123	1463.076501	18.793011
43.817073	1462.493710	18.798029
43.754123	1462.139146	18.803047
43.490949	1461.854474	18.808064
43.911784	1477.092140	18.813082
43.795724	1478.709262	18.818099
43.890395	1488.270352	18.823117
44.573065	1490.186724	18.828135
44.207178	1490.762017	18.833152
44.355978	1496.330478	18.838170
44.575544	1491.203713	18.843187
44.364736	1494.060534	18.848205
44.552934	1484.448053	18.853223
44.298106	1488.268704	18.858240
44.561252	1486.516348	18.863258
44.642545	1497.839642	18.868275
44.859384	1505.780584	18.873293
44.829664	1511.398234	18.878311
45.084859	1513.875338	18.883328
45.070567	1500.424999	18.888346
45.149645	1484.951259	18.893363
44.733268	1483.686731	18.898381
45.057357	1478.306708	18.903399
45.160992	1496.783759	18.908416
45.271683	1497.868994	18.913434
44.966693	1475.100123	18.918451
44.851958	1498.002992	18.923469
45.394566	1504.086810	18.928487
45.423882	1511.996744	18.933504
45.322547	1524.168823	18.938522
45.768619	1514.737301	18.943539
45.671608	1491.002081	18.948557
45.567120	1479.073343	18.953575
45.376054	1473.554860	18.958592
45.481225	1482.844171	18.963610
45.612128	1480.270088	18.968627
45.188398	1478.019514	18.973645
45.542683	1496.134128	18.978663
45.286618	1521.769258	18.983680
45.343020	1510.179606	18.988698
45.446242	1508.541457	18.993715
45.320030	1511.179015	18.998733
45.896395	1510.313152	19.003751
45.913697	1510.738521	19.008768
45.544748	1536.213811	19.013786
46.024060	1534.175959	19.018803
45.928546	1536.571474	19.023821
46.014774	1542.653766	19.028839
46.205701	1534.653376	19.033856
46.194522	1549.032907	19.038874
46.310665	1532.286043	19.043891
46.063419	1539.612449	19.048909
46.183854	1540.613411	19.053927
46.299533	1539.408180	19.058944
46.252574	1540.671024	19.063962
46.316397	1540.172888	19.068979
46.559283	1529.393234	19.073997
46.496349	1527.577451	19.079015
46.384517	1552.781571	19.084032
46.582963	1568.331827	19.089050
47.024604	1564.023932	19.094067
46.510995	1573.657841	19.099085
46.725655	1570.704203	19.104103
47.040880	1568.068548	19.109120
46.946069	1560.463740	19.114138
47.255654	1565.577566	19.119155
46.993847	1571.668177	19.124173
47.374377	1560.234345	19.129191
47.469624	1560.789336	19.134208
47.366965	1568.744727	19.139226
47.352191	1554.428593	19.144243
47.188205	1551.594018	19.149261
47.227776	1550.667665	19.154279
47.522462	1550.754128	19.159296
47.284502	1568.897020	19.164314
47.351368	1558.366089	19.169331
47.350682	1558.762940	19.174349
47.482613	1565.322859	19.179367
47.633449	1554.886700	19.184384
47.656312	1552.630417	19.189402
47.926021	1551.790229	19.194419
47.721357	1556.819764	19.199437
47.819924	1545.483514	19.204455
48.063660	1550.172450	19.209472
47.757128	1558.929727	19.214490
47.773764	1546.483942	19.219507
47.457376	1552.305649	19.224525
47.789314	1542.859707	19.229543
47.821974	1542.352550	19.234560
47.653842	1547.395333	19.239578
47.972776	1546.482453	19.244595
47.935920	1567.538164	19.249613
47.734223	1580.198658	19.254631
48.024481	1569.764446	19.259648
47.827408	1592.170304	19.264666
48.044560	1583.050155	19.269683
48.003558	1574.966433	19.274701
48.030286	1593.181346	19.279719
48.583407	1599.306373	19.284736
48.601556	1608.341280	19.289754
48.582788	1602.788373	19.294771
48.564932	1609.256346	19.299789
48.540112	1613.989286	19.304807
48.698218	1608.814182	19.309824
48.487659	1615.752919	19.314842
48.590218	1605.869119	19.319859
48.827021	1606.864044	19.324877
49.149467	1599.836045	19.329895
48.848186	1605.580877	19.334912
48.847089	1607.876559	19.339930
48.696415	1599.389350	19.344947
48.669743	1602.781041	19.349965
48.858143	1626.057967	19.354983
49.174307	1631.260480	19.360000
49.255631	1632.968409	19.365018
49.471898	1623.754497	19.370035
49.445361	1631.888063	19.375053
49.572378	1629.302197	19.380071
49.676920	1627.103459	19.385088
49.507439	1630.677789	19.390106
50.091262	1616.298700	19.395123
49.885061	1624.452111	19.400141
49.733264	1619.260506	19.405159
50.022803	1619.493864	19.410176
49.590138	1634.114952	19.415194
49.675093	1619.949382	19.420211
49.695953	1622.643747	19.425229
49.635483	1624.112149	19.430247
49.892810	1622.254061	19.435264
49.386185	1623.048061	19.440282
49.647077	1616.904520	19.445299
50.113474	1637.005035	19.450317
50.223115	1640.963698	19.455335
50.818767	1646.958307	19.460352
50.305084	1643.126522	19.465370
50.150785	1621.143647	19.470387
50.396186	1622.834893	19.475405
50.083257	1638.088081	19.480423
50.854350	1644.559734	19.485440
50.440463	1644.767619	19.490458
50.712592	1642.660854	19.495475
50.713358	1638.624586	19.500493
50.721326	1649.842212	19.505511
50.974111	1639.390329	19.510528
50.543855	1632.966163	19.515546
50.890315	1628.490933	19.520563
50.742688	1630.222918	19.525581
50.978326	1625.488086	19.530599
51.105844	1641.610889	19.535616
50.984070	1639.752461	19.540634
51.282073	1629.079165	19.545651
50.869118	1641.434507	19.550669
50.777850	1639.626149	19.555687
50.937080	1636.739722	19.560704
50.951063	1641.077727	19.565722
50.779963	1649.814249	19.570739
51.050594	1650.936050	19.575757
50.859788	1672.298408	19.580775
51.273718	1667.710850	19.585792
51.094168	1679.039788	19.590810
51.497005	1675.943435	19.595827
51.581597	1670.466915	19.600845
51.427190	1683.907373	19.605863
51.872029	1690.567981	19.610880
51.556982	1699.293481	19.615898
51.732994	1695.231978	19.620915
52.070131	1693.556140	19.625933
52.074482	1698.129188	19.630951
52.364509	1694.117734	19.635968
52.354553	1687.498516	19.640986
52.302167	1667.145569	19.646003
52.464853	1655.034964	19.651021
52.133885	1660.596754	19.656039
51.879658	1646.894635	19.661056
52.238142	1660.104668	19.666074
52.467274	1674.165311	19.671091
52.588492	1681.168135	19.676109
52.322550	1693.032946	19.681127
52.526376	1684.806163	19.686144
52.085419	1695.547683	19.691162
52.417225	1688.866084	19.696179
52.090862	1687.451641	19.701197
51.962381	1687.137818	19.706215
52.495134	1681.701002	19.711232
52.568148	1705.735210	19.716250
52.977572	1706.864390	19.721267
53.330207	1704.686841	19.726285
52.794112	1714.056870	19.731303
53.131210	1706.221190	19.736320
53.063393	1712.277830	19.741338
52.972611	1715.794495	19.746355
53.392978	1708.960870	19.751373
53.090630	1714.875778	19.756391
53.102199	1710.904626	19.761408
53.206589	1710.535591	19.766426
53.402423	1714.418423	19.771443
53.085840	1720.041629	19.776461
53.213828	1723.009414	19.781479
53.559228	1709.457137	19.786496
53.207294	1715.828214	19.791514
53.332148	1735.191894	19.796531
53.776661	1737.567287	19.801549
53.688670	1748.662867	19.806567
53.971720	1737.037756	19.811584
53.825057	1739.219537	19.816602
54.046685	1742.316126	19.821619
54.083228	1732.736424	19.826637
53.621647	1738.022618	19.831655
54.312344	1731.025232	19.836672
53.957362	1720.632394	19.841690
53.896971	1740.009174	19.846707
54.288865	1732.121517	19.851725
54.257553	1726.426955	19.856743
54.561031	1726.614317	19.861760
54.373600	1724.986582	19.866778
54.229902	1740.706726	19.871795
54.560513	1749.245058	19.876813
54.395082	1765.184145	19.881831
54.687432	1759.414240	19.886848
54.613346	1753.907620	19.891866
54.568871	1758.743250	19.896883
55.053631	1746.255769	19.901901
54.464697	1749.675846	19.906919
54.746592	1761.342910	19.911936
54.946105	1748.165647	19.916954
55.059592	1748.853440	19.921971
55.142877	1751.583176	19.926989
54.728656	1753.717453	19.932007
54.935667	1753.433611	19.937024
55.437886	1763.160568	19.942042
55.126841	1760.546097	19.947059
55.553379	1770.537503	19.952077
55.373250	1767.578012	19.957095
55.313420	1753.714753	19.962112
55.268721	1768.622601	19.967130
55.506926	1781.547928	19.972147
55.650424	1773.304102	19.977165
55.496800	1783.479171	19.982183
55.919091	1777.248863	19.987200
56.062491	1777.452443	19.992218
55.963326	1775.478268	19.997235
56.221260	1771.277436	20.002253
55.876468	1775.595445	20.007271
55.925816	1767.516571	20.012288
56.204463	1771.504419	20.017306
56.255993	1767.300693	20.022323
56.445073	1765.784927	20.027341
55.860674	1776.368339	20.032359
56.001516	1774.542669	20.037376
56.286808	1775.004066	20.042394
55.969366	1774.580342	20.047411
56.154735	1764.167269	20.052429
56.199331	1773.660640	20.057447
56.017138	1766.008760	20.062464
56.535959	1773.084488	20.067482
56.394881	1787.064696	20.072499
56.636487	1790.691393	20.077517
56.417103	1796.627855	20.082535
56.715788	1788.444980	20.087552
56.535543	1800.180372	20.092570
56.582676	1804.711936	20.097587
56.967306	1801.777997	20.102605
56.414328	1822.990005	20.107623
56.612348	1826.119051	20.112640
56.809247	1821.213417	20.117658
57.133642	1823.223089	20.122675
57.228805	1819.605374	20.127693
56.981511	1820.438606	20.132711
57.490510	1834.421853	20.137728
57.711140	1837.441469	20.142746
57.800859	1834.891847	20.147763
57.782169	1821.400817	20.152781
57.808617	1807.332921	20.157799
57.634332	1808.917775	20.162816
57.806665	1814.429911	20.167834
57.733743	1814.656838	20.172851
57.793425	1816.769891	20.177869
57.816994	1837.221174	20.182887
57.885241	1841.037731	20.187904
58.077046	1837.310943	20.192922
57.941449	1846.974474	20.197939
57.942016	1841.005737	20.202957
58.501152	1844.926784	20.207975
58.064287	1844.498386	20.212992
58.266963	1841.533884	20.218010
58.297497	1839.464457	20.223027
58.395981	1836.719905	20.228045
58.536628	1841.256498	20.233063
58.435558	1840.410645	20.238080
58.309321	1840.360590	20.243098
58.155494	1837.914591	20.248115
58.247967	1851.775565	20.253133
58.377491	1858.325772	20.258151
58.734536	1868.471818	20.263168
58.800726	1871.735441	20.268186
58.521748	1864.085728	20.273203
58.823809	1866.750595	20.278221
59.022991	1887.748843	20.283239
59.225008	1899.985054	20.288256
59.415258	1891.755877	20.293274
59.472206	1900.247597	20.298291
59.444613	1883.172176	20.303309
59.477026	1869.161499	20.308327
59.178374	1865.629517	20.313344
59.394963	1872.700320	20.318362
59.654623	1883.285451	20.323379
59.563800	1886.539200	20.328397
59.920710	1886.840555	20.333415
59.688978	1886.269215	20.338432
59.756076	1887.997041	20.343450
59.895775	1882.802252	20.348467
59.818736	1889.426169	20.353485
59.753259	1885.550962	20.358503
59.782908	1885.302135	20.363520
59.809361	1888.617598	20.368538
59.726276	1883.818242	20.373555
59.892335	1899.318286	20.378573
59.951254	1893.652645	20.383591
60.072641	1922.107823	20.388608
60.274162	1912.120672	20.393626
60.164375	1925.439020	20.398643
60.464769	1921.377965	20.403661
60.471487	1924.439049	20.408679
60.516467	1919.311468	20.413696
60.520423	1906.132138	20.418714
60.655794	1915.793253	20.423731
60.725965	1913.345065	20.428749
60.788700	1908.600534	20.433767
61.011260	1917.000337	20.438784
60.653096	1907.258218	20.443802
60.662939	1929.677612	20.448819
61.001996	1932.141518	20.453837
61.106420	1934.599123	20.458855
61.118680	1941.230941	20.463872
61.525204	1933.380720	20.468890
61.389621	1939.829118	20.473907
61.369838	1928.789672	20.478925
61.544611	1934.121350	20.483943
61.463692	1937.845467	20.488960
61.717281	1929.391655	20.493978
61.814060	1936.571842	20.498995
61.655062	1924.243741	20.504013
61.753429	1924.551210	20.509031
61.554040	1932.254299	20.514048
61.710489	1930.564008	20.519066
61.771286	1935.778907	20.524083
61.894391	1958.919112	20.529101
61.837658	1952.805683	20.534119
62.036423	1963.113169	20.539136
62.217828	1962.385377	20.544154
62.008149	1956.319265	20.549171
61.919249	1969.262980	20.554189
62.104997	1966.422892	20.559207
61.998742	1970.399995	20.564224
62.377075	1978.459756	20.569242
62.810705	1980.127024	20.574259
62.733655	1982.137512	20.579277
63.232114	1978.289158	20.584295
62.754381	1981.681264	20.589312
63.226070	1977.066947	20.594330
62.982332	1975.210326	20.599347
62.962023	1986.031535	20.604365
63.028938	1984.530031	20.609383
62.898363	1973.972393	20.614400
62.900670	1977.653046	20.619418
62.998542	1980.785683	20.624435
62.562764	1971.513188	20.629453
62.810634	1979.863376	20.634471
62.753070	1978.677882	20.639488
63.333739	1990.049123	20.644506
63.224895	2010.870905	20.649523
63.127972	2009.323842	20.654541
63.490452	2015.876365	20.659559
62.904542	2007.810026	20.664576
63.507014	2012.953352	20.669594
63.369002	2030.897219	20.674611
63.670548	2034.993152	20.679629
63.762031	2031.850946	20.684647
63.394570	2044.163268	20.689664
63.565195	2033.922904	20.694682
63.695029	2054.370693	20.699699
64.587977	2065.395339	20.704717
64.589287	2056.385176	20.709735
64.528195	2067.405091	20.714752
64.808881	2052.526732	20.719770
64.413695	2045.410841	20.724787
64.618417	2029.144417	20.729805
64.738734	2028.909342	20.734823
64.574629	2042.664871	20.739840
65.007587	2036.264015	20.744858
64.466178	2037.834565	20.749875
64.441607	2049.209024	20.754893
65.114576	2060.521762	20.759911
64.922666	2067.419041	20.764928
65.172339	2049.905336	20.769946
64.846817	2058.826449	20.774963
65.252131	2051.707198	20.779981
65.515459	2060.577065	20.784999
65.137784	2063.467862	20.790016
64.895059	2055.924846	20.795034
65.348115	2056.093400	20.800051
64.700712	2059.170879	20.805069
65.159309	2065.303842	20.810087
65.602483	2075.498976	20.815104
66.087052	2071.326551	20.820122
65.695580	2071.503572	20.825139
65.543575	2083.840159	20.830157
66.170865	2070.223860	20.835175
65.833646	2076.760156	20.840192
66.101598	2086.764590	20.845210
66.346870	2073.368486	20.850227
66.144740	2081.387227	20.855245
66.561462	2073.581703	20.860263
66.228955	2077.445449	20.865280
66.786513	2069.438524	20.870298
66.350470	2071.562473	20.875315
66.226009	2076.470075	20.880333
66.548966	2064.888118	20.885351
66.128733	2071.781204	20.890368
66.567944	2081.602430	20.895386
66.471449	2092.168220	20.900403
66.561937	2102.503533	20.905421
66.865643	2105.249659	20.910439
66.553974	2115.994709	20.915456
66.653374	2108.039459	20.920474
66.665444	2106.662545	20.925491
66.570905	2123.838390	20.930509
67.335761	2123.598371	20.935527
67.013327	2130.706992	20.940544
67.333807	2132.453403	20.945562
67.389011	2122.688110	20.950579
67.501058	2134.986024	20.955597
67.804116	2125.152414	20.960615
67.622837	2135.086245	20.965632
67.592744	2131.689530	20.970650
67.545244	2126.422060	20.975667
67.303137	2133.894536	20.980685
67.924615	2123.988034	20.985703
67.712876	2120.553628	20.990720
68.260537	2126.430781	20.995738
67.853700	2118.287159	21.000755
67.878086	2143.246529	21.005773
68.081960	2147.260807	21.010791
68.084779	2157.346300	21.015808
68.252326	2150.977249	21.020826
68.553764	2155.888507	21.025843
68.254091	2160.581805	21.030861
68.287936	2155.732731	21.035879
68.399877	2163.562817	21.040896
68.272276	2160.461511	21.045914
68.605455	2155.257491	21.050931
68.421580	2170.878029	21.055949
68.676396	2172.069012	21.060967
68.801153	2172.290244	21.065984
69.306699	2177.358116	21.071002
69.391219	2174.398511	21.076019
69.292642	2170.722974	21.081037
69.495242	2169.648593	21.086055
69.254542	2165.410970	21.091072
69.317315	2168.112873	21.096090
69.340305	2173.488022	21.101107
69.175670	2163.306319	21.106125
69.499612	2166.676019	21.111143
69.362638	2166.604707	21.116160
69.510779	2173.363959	21.121178
69.896534	2186.639618	21.126195
69.564097	2189.270034	21.131213
69.932706	2180.015658	21.136231
70.072135	2191.359184	21.141248
69.928001	2198.466519	21.146266
70.258515	2191.241073	21.151283
70.323057	2195.891519	21.156301
70.363033	2184.466460	21.161319
70.634769	2195.290733	21.166336
70.374681	2185.798543	21.171354
70.728210	2181.521771	21.176371
70.669492	2191.655640	21.181389
70.265034	2187.396454	21.186407
70.824209	2186.533005	21.191424
70.667151	2190.561076	21.196442
70.786084	2187.003121	21.201459
70.501210	2181.235342	21.206477
70.657627	2192.850249	21.211495
70.507408	2212.846149	21.216512
70.643044	2220.841821	21.221530
71.092057	2219.181100	21.226547
70.728492	2218.705933	21.231565
71.015626	2224.551970	21.236583
71.189170	2246.599531	21.241600
71.026369	2247.839452	21.246618
71.480302	2251.011920	21.251635
71.444062	2254.374826	21.256653
71.246681	2246.572080	21.261671
71.328269	2259.863029	21.266688
71.723599	2265.500668	21.271706
72.009737	2276.848161	21.276723
71.866892	2279.126229	21.281741
71.780787	2269.796165	21.286759
72.243690	2275.976725	21.291776
71.951260	2279.420944	21.296794
72.163722	2273.461705	21.301811
72.123615	2270.236087	21.306829
72.029139	2253.802549	21.311847
72.084761	2280.107642	21.316864
72.083834	2299.698704	21.321882
72.354425	2291.357426	21.326899
72.067129	2303.936406	21.331917
72.412613	2297.494588	21.336935
72.890342	2289.512551	21.341952
72.630883	2308.104312	21.346970
72.988847	2314.350256	21.351987
73.181311	2322.895203	21.357005
73.532855	2319.880816	21.362023
73.679133	2317.979585	21.367040
73.392052	2305.973498	21.372058
73.473085	2290.266758	21.377075
73.553136	2286.580768	21.382093
73.453951	2283.504661	21.387111
73.543706	2274.050660	21.392128
73.861222	2270.892313	21.397146
73.856775	2270.604040	21.402163
73.712677	2281.481932	21.407181
73.828344	2295.959496	21.412199
73.921923	2314.543119	21.417216
74.090997	2306.188886	21.422234
74.148287	2307.627462	21.427251
74.234587	2310.431005	21.432269
74.152274	2311.629878	21.437287
73.984190	2311.455447	21.442304
73.605220	2311.012741	21.447322
74.169897	2309.968670	21.452339
74.073118	2321.597759	21.457357
74.079306	2329.291481	21.462375
74.367210	2345.309195	21.467392
74.175721	2342.936065	21.472410
74.552703	2338.562863	21.477427
74.685798	2341.317934	21.482445
75.294774	2348.160942	21.487463
75.871710	2345.146704	21.492480
75.276049	2337.108177	21.497498
75.516783	2328.851924	21.502515
75.173963	2325.654861	21.507533
75.251330	2323.482364	21.512551
75.374011	2323.665952	21.517568
75.306220	2334.137999	21.522586
75.637014	2350.122649	21.527603
75.647777	2358.066396	21.532621
75.745508	2354.562099	21.537639
75.747619	2344.497591	21.542656
75.686562	2355.300007	21.547674
75.910618	2345.505688	21.552691
75.568866	2352.817191	21.557709
75.768885	2352.153426	21.562727
75.975587	2350.460101	21.567744
75.857991	2362.830394	21.572762
76.087808	2373.669199	21.577779
76.181637	2382.300945	21.582797
76.195386	2384.125234	21.587815
76.561988	2379.369122	21.592832
76.400184	2376.696224	21.597850
76.761201	2378.807195	21.602867
76.283527	2369.605352	21.607885
76.609372	2393.569722	21.612903
76.990213	2402.667592	21.617920
77.227451	2402.585029	21.622938
77.204426	2401.402652	21.627955
77.185117	2401.131004	21.632973
77.055999	2404.786236	21.637991
77.326914	2397.562079	21.643008
77.075869	2405.469788	21.648026
77.367427	2395.533585	21.653043
77.052104	2402.211661	21.658061
77.387175	2396.720658	21.663079
77.352549	2408.327339	21.668096
77.620369	2427.495641	21.673114
77.843486	2436.202699	21.678131
77.927647	2433.153740	21.683149
77.742068	2434.585613	21.688167
78.210238	2432.971505	21.693184
77.980033	2432.920321	21.698202
77.949372	2427.667286	21.703219
78.200067	2432.091389	21.708237
78.373243	2429.017093	21.713255
78.308897	2431.715444	21.718272
78.234937	2439.406325	21.723290
78.477350	2445.687164	21.728307
78.872499	2450.028351	21.733325
79.057285	2455.376665	21.738343
79.136313	2449.893113	21.743360
79.097689	2456.065880	21.748378
79.144020	2453.207406	21.753395
79.108626	2451.933573	21.758413
78.900503	2458.477631	21.763431
78.949180	2459.404495	21.768448
78.697247	2449.345091	21.773466
78.748717	2452.741967	21.778483
78.989595	2465.179080	21.783501
78.594915	2480.703870	21.788519
79.148648	2488.129450	21.793536
79.427691	2505.298510	21.798554
79.475557	2502.027993	21.803571
79.857725	2516.944761	21.808589
80.020123	2516.957826	21.813607
80.435680	2506.182028	21.818624
80.483004	2518.415162	21.823642
80.481077	2511.595066	21.828659
80.194170	2504.734079	21.833677
80.328105	2501.754238	21.838695
80.151818	2502.827523	21.843712
79.804421	2510.699242	21.848730
80.667371	2517.196248	21.853747
80.768423	2532.282112	21.858765
80.800842	2539.810396	21.863783
81.522151	2522.344590	21.868800
81.289866	2507.723972	21.873818
81.125511	2492.472111	21.878835
81.215534	2489.161562	21.883853
81.186047	2483.406385	21.888871
81.521379	2477.851536	21.893888
81.151166	2477.201881	21.898906
81.420637	2498.666082	21.903923
81.523115	2509.198491	21.908941
81.358465	2522.799430	21.913959
81.988209	2517.361455	21.918976
81.716957	2522.523359	21.923994
81.732696	2528.514547	21.929011
82.080939	2513.452745	21.934029
81.670287	2525.558822	21.939047
82.168460	2518.556682	21.944064
81.893532	2520.830038	21.949082
81.817977	2525.669075	21.954099
82.059462	2513.256215	21.959117
81.865493	2528.670727	21.964135
82.132277	2536.173864	21.969152
81.783649	2528.990018	21.974170
82.040049	2547.757828	21.979187
82.456448	2559.173369	21.984205
81.998556	2562.901665	21.989223
82.178225	2565.634515	21.994240
82.319829	2567.954198	21.999258
82.591261	2585.013392	22.004275
82.794349	2596.947640	22.009293
82.870903	2588.671531	22.014311
82.819285	2593.148588	22.019328
82.817079	2603.188946	22.024346
83.258035	2609.315793	22.029363
83.544713	2613.810572	22.034381
83.399570	2619.875425	22.039399
83.864801	2624.492069	22.044416
83.896450	2619.623529	22.049434
83.951225	2610.195574	22.054451
84.261990	2613.465000	22.059469
84.046123	2625.508064	22.064487
84.377944	2607.407751	22.069504
84.093600	2612.133098	22.074522
84.453302	2611.153980	22.079539
84.599862	2611.073802	22.084557
84.420478	2610.289859	22.089575
84.522815	2618.007598	22.094592
84.581275	2615.284482	22.099610
84.546933	2604.436316	22.104627
84.867990	2606.316143	22.109645
84.761630	2613.142642	22.114663
84.438882	2612.539071	22.119680
84.497129	2624.183319	22.124698
84.793042	2632.881412	22.129715
85.222131	2638.803356	22.134733
84.973212	2635.493669	22.139751
84.856478	2639.206158	22.144768
85.387307	2655.831254	22.149786
85.274989	2656.682772	22.154803
85.856143	2663.129562	22.159821
85.431906	2667.558181	22.164839
85.828639	2660.267839	22.169856
85.891751	2669.646899	22.174874
86.097277	2665.764900	22.179891
86.268806	2660.251816	22.184909
85.700538	2674.167598	22.189927
86.352829	2669.383087	22.194944
86.704159	2689.714415	22.199962
86.600157	2693.923206	22.204979
86.466314	2683.821695	22.209997
86.551302	2687.824070	22.215015
86.733028	2690.958546	22.220032
86.784719	2693.067725	22.225050
86.728666	2686.387000	22.230067
86.961489	2679.290456	22.235085
86.994293	2689.746711	22.240103
86.932040	2678.577142	22.245120
87.016173	2681.800966	22.250138
86.953724	2688.962543	22.255155
86.874269	2698.589377	22.260173
87.103610	2714.481334	22.265191
87.240383	2708.647421	22.270208
87.393433	2723.312701	22.275226
87.154192	2728.634333	22.280243
87.725410	2728.121604	22.285261
87.912157	2738.970933	22.290279
87.919958	2738.637126	22.295296
88.008837	2734.830681	22.300314
88.113543	2743.751169	22.305331
88.249879	2731.555891	22.310349
88.186958	2752.040000	22.315367
88.161122	2732.450703	22.320384
88.190511	2733.400258	22.325402
88.548111	2759.240152	22.330419
88.715997	2763.717401	22.335437
88.742646	2768.181379	22.340455
88.728851	2774.873959	22.345472
88.976171	2764.806649	22.350490
88.783680	2777.491403	22.355507
89.050956	2764.955977	22.360525
89.083232	2766.319206	22.365543
89.115833	2770.542058	22.370560
89.092938	2766.765098	22.375578
88.654934	2774.007275	22.380595
89.088455	2774.027898	22.385613
89.311585	2780.821874	22.390631
89.108663	2791.276601	22.395648
89.526780	2799.158380	22.400666
89.551960	2822.443613	22.405683
89.941795	2822.108877	22.410701
89.961079	2829.910915	22.415719
90.056036	2822.962277	22.420736
90.270654	2825.740183	22.425754
90.196689	2819.865466	22.430771
90.282304	2816.378027	22.435789
90.285966	2829.976027	22.440807
90.638985	2834.994329	22.445824
90.825650	2839.588964	22.450842
90.970540	2858.325580	22.455859
91.074924	2850.180160	22.460877
90.876865	2845.603429	22.465895
90.899328	2846.833648	22.470912
91.495215	2839.443979	22.475930
91.501492	2848.281978	22.480947
91.439345	2840.299900	22.485965
91.454215	2849.045146	22.490983
91.177255	2839.532506	22.496000
91.466636	2837.397931	22.501018
91.361941	2841.855289	22.506035
91.127249	2850.171720	22.511053
91.661023	2855.501480	22.516071
91.429369	2862.884000	22.521088
91.726701	2867.216275	22.526106
91.712604	2887.134256	22.531123
91.917837	2885.941879	22.536141
92.349278	2886.572265	22.541159
92.387528	2894.365689	22.546176
92.415917	2885.979671	22.551194
92.426486	2894.698489	22.556211
93.116759	2903.423101	22.561229
93.330709	2895.408756	22.566247
92.948943	2891.956801	22.571264
92.926426	2895.745116	22.576282
92.788307	2905.998671	22.581299
93.395745	2916.707353	22.586317
93.485639	2915.197041	22.591335
93.528039	2920.693055	22.596352
93.703633	2916.691537	22.601370
93.609207	2902.874889	22.606387
93.585969	2906.000760	22.611405
94.306245	2916.035711	22.616423
93.791688	2910.135343	22.621440
94.407083	2903.206965	22.626458
93.941451	2903.932832	22.631475
93.943178	2911.844106	22.636493
94.116026	2911.366099	22.641511
94.135791	2903.916882	22.646528
94.183814	2905.362557	22.651546
94.240615	2914.095793	22.656563
94.482507	2926.628185	22.661581
94.516247	2935.668773	22.666599
94.508822	2940.051820	22.671616
94.611001	2926.632565	22.676634
94.565637	2942.376064	22.681651
94.929546	2928.832853	22.686669
94.840800	2939.445183	22.691687
94.888067	2959.111789	22.696704
94.959308	2956.819947	22.701722
95.100007	2966.430646	22.706739
95.527109	2964.391796	22.711757
95.621198	2955.091381	22.716775
95.195959	2973.768810	22.721792
95.381886	2980.288720	22.726810
95.399325	2978.758486	22.731827
95.405788	2984.122278	22.736845
95.186304	3000.189871	22.741863
95.400963	3017.917164	22.746880
96.279039	3020.129589	22.751898
96.018392	3023.073463	22.756915
96.691539	3004.145060	22.761933
96.855710	3008.678898	22.766951
96.621714	3025.185116	22.771968
97.243577	3023.156594	22.776986
96.883487	3022.278085	22.782003
97.210177	3027.629133	22.787021
97.216636	3031.722917	22.792039
96.900579	3043.927933	22.797056
97.394527	3034.297629	22.802074
97.398309	3037.819045	22.807091
97.324116	3033.402492	22.812109
97.518269	3034.642937	22.817127
97.266316	3037.657421	22.822144
97.554667	3021.140517	22.827162
97.814970	3033.554999	22.832179
97.683576	3061.541469	22.837197
98.150606	3063.174211	22.842215
98.090088	3068.361312	22.847232
97.966077	3064.093921	22.852250
98.047681	3066.530873	22.857267
98.299626	3070.064044	22.862285
98.643719	3076.181889	22.867303
98.194539	3070.315536	22.872320
98.570562	3087.746571	22.877338
98.404267	3092.803527	22.882355
98.549177	3102.900998	22.887373
98.712356	3094.417400	22.892391
98.935342	3100.173391	22.897408
99.207728	3112.956792	22.902426
99.098284	3115.983962	22.907443
99.260772	3119.239810	22.912461
100.049200	3109.682843	22.917479
99.764340	3125.684205	22.922496
99.962992	3114.686161	22.927514
99.459116	3119.867016	22.932531
99.749211	3113.959193	22.937549
100.226872	3117.686959	22.942567
100.177588	3122.768683	22.947584
99.940698	3118.116794	22.952602
100.051830	3131.196531	22.957619
100.114697	3141.595764	22.962637
100.612821	3136.983433	22.967655
100.597378	3144.576415	22.972672
100.527805	3137.306410	22.977690
100.633799	3147.159169	22.982707
100.694551	3149.910593	22.987725
100.932908	3161.268209	22.992743
100.803977	3175.785244	22.997760
100.647566	3170.012990	23.002778
101.116155	3170.412455	23.007795
101.021447	3169.943219	23.012813
101.440379	3184.934282	23.017831
101.477534	3200.295128	23.022848
101.757276	3195.076760	23.027866
101.891794	3194.112574	23.032883
102.002372	3192.392525	23.037901
102.051717	3188.965325	23.042919
101.785907	3195.249350	23.047936
101.912675	3191.024735	23.052954
101.818043	3194.908501	23.057971
102.023505	3210.943100	23.062989
102.190966	3224.065574	23.068007
102.117166	3221.284288	23.073024
102.275670	3224.357752	23.078042
102.315948	3222.698134	23.083059
102.885649	3255.364635	23.088077
102.963123	3244.429829	23.093095
103.060366	3247.913016	23.098112
103.161167	3247.282342	23.103130
103.381542	3242.480449	23.108147
103.335680	3239.502816	23.113165
103.523994	3236.832935	23.118183
103.464931	3252.740033	23.123200
103.555616	3271.904993	23.128218
103.787163	3266.296938	23.133235
103.917920	3272.469010	23.138253
104.038164	3268.075771	23.143271
103.662643	3277.628267	23.148288
104.312438	3287.583379	23.153306
104.386203	3280.195923	23.158323
104.383197	3301.344462	23.163341
104.662295	3299.022947	23.168359
104.462988	3301.579974	23.173376
104.781649	3304.434475	23.178394
105.149250	3295.703214	23.183411
104.711755	3288.227404	23.188429
105.058865	3294.901911	23.193447
104.907178	3305.267810	23.198464
105.396269	3319.471839	23.203482
105.594818	3326.994511	23.208499
105.460377	3331.020713	23.213517
105.514773	3322.175840	23.218535
105.769616	3326.601485	23.223552
105.595532	3323.658015	23.228570
105.663301	3321.526137	23.233587
105.659719	3337.322187	23.238605
105.827508	3336.388321	23.243623
105.958715	3344.593768	23.248640
106.125297	3345.008891	23.253658
106.364084	3338.650416	23.258675
106.024140	3350.473014	23.263693
106.580879	3374.228317	23.268711
106.703553	3381.478913	23.273728
106.517081	3381.022865	23.278746
106.584224	3373.933304	23.283763
106.782459	3393.745986	23.288781
106.846301	3390.380518	23.293799
107.015625	3409.466514	23.298816
107.215912	3402.388403	23.303834
107.403687	3405.171245	23.308851
107.457423	3431.482938	23.313869
107.412766	3431.944779	23.318887
107.611143	3433.508176	23.323904
107.755418	3432.451027	23.328922
107.918784	3427.846290	23.333939
108.194520	3454.569757	23.338957
107.971879	3444.430847	23.343975
108.319064	3455.312436	23.348992
108.180059	3459.387850	23.354010
108.387386	3456.647468	23.359027
108.365307	3456.258347	23.364045
108.427364	3465.814636	23.369063
108.916284	3477.419267	23.374080
109.170404	3479.119520	23.379098
109.427222	3484.391723	23.384115
109.180697	3485.381011	23.389133
109.240535	3466.856537	23.394151
109.297706	3479.027387	23.399168
109.328780	3475.513380	23.404186
109.371226	3474.722263	23.409203
109.182853	3499.168195	23.414221
109.676030	3498.102601	23.419239
109.848980	3508.985460	23.424256
109.763807	3504.756411	23.429274
109.874980	3513.793595	23.434291
110.063502	3539.071398	23.439309
110.390028	3527.471623	23.444327
110.642681	3537.462206	23.449344
110.206099	3543.103729	23.454362
110.596147	3536.293018	23.459379
110.653414	3563.482690	23.464397
110.660322	3559.873839	23.469415
110.974961	3559.423565	23.474432
110.920002	3562.087096	23.479450
111.224079	3581.789616	23.484467
111.090965	3589.864461	23.489485
111.755282	3589.511917	23.494503
111.606450	3593.627571	23.499520
111.596820	3586.347057	23.504538
112.060815	3586.571312	23.509555
112.093164	3590.703090	23.514573
112.087656	3582.285683	23.519591
112.088818	3592.172188	23.524608
112.157615	3603.328621	23.529626
112.330059	3613.067941	23.534643
112.949464	3619.639327	23.539661
113.038105	3606.955183	23.544679
112.850946	3612.637800	23.549696
112.918725	3619.112541	23.554714
113.402671	3606.192606	23.559731
113.029516	3615.799642	23.564749
113.104483	3611.383867	23.569767
113.452625	3608.221374	23.574784
113.272180	3623.523713	23.579802
113.440569	3627.277118	23.584819
113.507967	3639.915694	23.589837
113.689024	3641.076857	23.594855
113.598725	3643.173802	23.599872
113.766495	3651.537937	23.604890
114.165954	3653.942933	23.609907
114.329930	3669.492736	23.614925
114.527513	3663.331883	23.619943
114.599968	3672.618077	23.624960
114.651499	3663.171516	23.629978
114.699544	3659.165687	23.634995
114.641624	3669.823422	23.640013
114.452385	3668.280027	23.645031
114.853887	3681.479966	23.650048
114.933204	3695.215043	23.655066
115.290839	3681.824577	23.660083
114.954768	3695.253489	23.665101
115.128270	3706.745845	23.670119
115.499287	3720.646131	23.675136
115.233186	3720.316223	23.680154
115.780996	3718.063238	23.685171
115.743298	3724.259388	23.690189
115.984119	3746.123758	23.695207
116.263426	3755.168341	23.700224
116.126694	3753.394213	23.705242
116.644761	3758.223340	23.710259
116.491383	3756.291726	23.715277
116.571592	3746.171080	23.720295
116.767891	3753.291180	23.725312
116.426374	3750.545374	23.730330
117.155973	3759.214765	23.735347
117.005231	3775.634399	23.740365
116.824157	3771.293170	23.745383
117.238426	3767.072468	23.750400
117.056669	3775.418047	23.755418
117.414369	3764.010584	23.760435
117.134232	3789.572930	23.765453
117.225116	3797.915202	23.770471
117.621204	3796.022712	23.775488
117.664073	3799.860286	23.780506
117.717749	3813.979630	23.785523
118.322529	3823.746070	23.790541
118.008923	3821.642496	23.795559
118.471377	3829.975357	23.800576
118.439054	3846.542035	23.805594
118.690704	3853.282165	23.810611
118.910821	3858.318039	23.815629
118.709134	3852.962071	23.820647
118.690157	3850.425159	23.825664
118.928805	3864.734852	23.830682
119.187072	3883.157908	23.835699
119.351085	3882.857319	23.840717
119.500200	3876.397694	23.845735
119.835486	3872.141983	23.850752
119.720515	3891.185390	23.855770
119.817073	3905.777659	23.860787
119.798832	3906.115856	23.865805
119.880944	3917.056531	23.870823
120.019734	3902.616982	23.875840
120.258613	3920.410993	23.880858
120.525663	3930.797882	23.885875
120.781050	3941.617422	23.890893
120.737387	3933.225814	23.895911
120.889127	3933.325685	23.900928
120.888237	3947.918347	23.905946
121.144319	3940.765812	23.910963
121.648540	3953.027340	23.915981
121.538003	3959.445072	23.920999
121.878045	3955.333831	23.926016
121.662364	3960.001583	23.931034
122.101973	3955.075450	23.936051
122.311240	3957.243806	23.941069
122.380125	3962.368090	23.946087
122.801851	3943.517891	23.951104
122.230330	3956.272928	23.956122
122.671110	3951.330460	23.961139
122.436280	3958.673865	23.966157
122.174371	3962.989407	23.971175
122.447695	3960.044722	23.976192
122.652805	3970.586364	23.981210
122.694595	3982.764481	23.986227
122.485674	3984.850363	23.991245
122.426835	4005.198440	23.996263
123.067720	4015.355501	24.001280
122.612927	4026.195202	24.006298
122.852843	4037.155951	24.011315
123.374888	4046.203509	24.016333
123.458152	4059.391392	24.021351
123.848356	4063.244475	24.026368
123.868937	4088.882427	24.031386
123.978563	4072.026216	24.036403
124.114003	4076.075340	24.041421
124.133097	4077.469997	24.046439
124.746839	4081.992466	24.051456
124.410801	4105.399942	24.056474
124.508362	4098.363295	24.061491
124.736465	4105.836973	24.066509
124.725593	4115.919112	24.071527
124.987169	4110.188467	24.076544
124.961382	4125.949616	24.081562
125.212509	4138.605877	24.086579
125.661546	4138.244408	24.091597
125.583001	4147.106611	24.096615
126.123465	4130.494511	24.101632
126.032724	4132.613248	24.106650
125.575615	4144.075479	24.111667
125.983499	4152.754156	24.116685
126.159432	4149.088892	24.121703
126.228085	4156.323580	24.126720
126.219156	4153.405418	24.131738
126.412478	4176.068424	24.136755
126.560800	4185.665234	24.141773
126.747132	4186.355474	24.146791
126.926807	4184.842804	24.151808
127.398189	4202.032953	24.156826
127.164954	4204.235877	24.161843
127.604848	4211.668705	24.166861
127.737882	4207.078594	24.171879
127.726250	4210.170525	24.176896
127.631220	4216.073184	24.181914
127.536803	4214.501861	24.186931
127.795885	4235.862311	24.191949
127.903695	4235.967868	24.196967
128.384672	4246.286549	24.201984
128.137017	4243.517270	24.207002
128.238011	4260.495053	24.212019
128.472890	4267.447197	24.217037
128.539511	4266.587870	24.222055
128.727712	4277.381343	24.227072
128.674150	4288.932123	24.232090
129.136884	4296.884467	24.237107
129.449696	4288.400693	24.242125
129.356194	4308.267471	24.247143
129.388338	4318.462718	24.252160
129.916126	4321.555307	24.257178
129.960595	4320.098825	24.262195
130.107692	4315.114216	24.267213
129.936395	4319.402284	24.272231
130.174742	4325.094774	24.277248
130.518915	4344.760535	24.282266
130.557747	4346.898444	24.287283
130.890405	4342.029629	24.292301
130.655203	4338.903535	24.297319
131.100552	4340.162820	24.302336
131.223229	4347.435522	24.307354
131.048675	4351.390658	24.312371
131.465303	4360.090449	24.317389
131.024802	4371.269774	24.322407
131.434977	4373.783355	24.327424
131.522725	4381.301619	24.332442
131.446116	4394.249655	24.337459
131.987600	4394.478446	24.342477
131.948243	4405.576550	24.347495
132.013759	4391.229369	24.352512
132.717919	4400.871876	24.357530
132.556413	4423.524184	24.362547
132.797507	4417.238123	24.367565
132.855862	4416.294717	24.372583
133.284317	4425.759557	24.377600
132.963426	4428.904993	24.382618
132.894893	4435.362440	24.387635
133.161133	4423.221936	24.392653
132.977015	4428.733077	24.397671
133.343998	4436.515479	24.402688
133.354283	4461.474610	24.407706
133.109827	4469.491925	24.412723
133.542609	4463.460801	24.417741
133.656611	4487.712643	24.422759
133.838523	4480.745355	24.427776
134.141754	4486.950833	24.432794
133.923350	4517.430805	24.437811
134.349535	4514.374928	24.442829
134.557430	4510.024735	24.447847
134.706001	4531.547166	24.452864
135.038655	4526.856651	24.457882
134.897503	4537.344075	24.462899
135.221534	4531.831316	24.467917
135.579823	4534.914552	24.472935
135.684846	4533.343314	24.477952
135.809794	4546.759382	24.482970
135.862488	4555.831246	24.487987
136.217680	4549.881024	24.493005
136.275090	4570.645300	24.498023
136.688282	4550.728397	24.503040
137.061175	4551.483108	24.508058
136.596599	4569.266137	24.513075
136.944813	4560.320829	24.518093
136.714921	4560.151855	24.523111
136.791994	4555.753970	24.528128
136.659913	4560.796691	24.533146
136.553902	4575.986084	24.538163
136.970795	4581.112521	24.543181
137.086939	4601.165124	24.548199
137.066154	4613.336749	24.553216
137.130143	4616.789910	24.558234
137.317389	4625.053314	24.563251
138.450517	4628.117207	24.568269
138.711473	4627.986426	24.573287
138.732272	4635.259953	24.578304
138.726814	4626.602982	24.583322
138.528498	4620.731986	24.588339
138.951523	4627.909912	24.593357
139.152326	4636.070289	24.598375
139.340317	4629.319660	24.603392
139.390437	4641.175636	24.608410
139.302824	4651.955097	24.613427
139.565140	4650.244464	24.618445
139.364691	4663.248228	24.623463
139.736347	4653.754864	24.628480
139.815960	4656.205782	24.633498
139.639984	4669.005100	24.638515
140.165679	4678.509543	24.643533
139.987825	4692.558090	24.648551
139.973936	4690.130444	24.653568
140.164555	4699.035892	24.658586
140.104972	4718.747185	24.663603
140.386400	4714.422583	24.668621
140.768903	4742.454728	24.673639
140.605559	4746.969961	24.678656
141.009382	4748.447969	24.683674
141.168749	4762.879865	24.688691
141.576337	4773.501596	24.693709
141.849337	4783.228185	24.698727
141.803245	4774.515636	24.703744
142.153703	4773.521581	24.708762
141.779597	4780.483629	24.713779
141.836046	4784.348339	24.718797
141.922288	4801.980377	24.723815
142.361757	4802.774105	24.728832
142.652761	4801.985555	24.733850
142.384070	4817.168596	24.738867
142.518924	4825.960487	24.743885
142.707450	4838.040611	24.748903
142.708313	4837.047620	24.753920
143.196359	4846.298131	24.758938
143.252671	4863.941090	24.763955
143.422316	4862.485924	24.768973
143.390006	4868.970243	24.773991
143.620640	4887.335270	24.779008
143.840911	4882.450605	24.784026
143.908980	4895.210964	24.789043
144.051074	4889.044624	24.794061
143.874717	4913.749468	24.799079
144.445493	4932.236706	24.804096
144.725292	4919.056881	24.809114
144.849325	4937.382096	24.814131
145.082071	4957.340687	24.819149
145.113639	4955.003528	24.824167
145.306609	4957.003051	24.829184
145.734741	4948.966046	24.834202
145.578741	4959.427070	24.839219
145.615592	4970.637797	24.844237
145.912783	4982.035456	24.849255
145.879160	4971.192212	24.854272
146.279999	4974.176373	24.859290
146.220839	5003.781303	24.864307
146.432029	5002.762998	24.869325
146.326389	5000.139422	24.874343
146.265430	5016.505757	24.879360
146.972683	5026.502901	24.884378
146.592181	5036.752625	24.889395
147.225821	5038.392312	24.894413
147.664459	5043.339705	24.899431
147.962925	5056.004642	24.904448
147.732862	5063.734423	24.909466
147.771779	5063.674190	24.914483
148.201130	5052.201192	24.919501
148.298961	5060.102797	24.924519
148.358096	5052.717314	24.929536
148.592017	5064.675929	24.934554
148.587555	5082.447692	24.939571
148.755185	5077.986268	24.944589
148.827943	5083.007910	24.949607
148.536598	5097.059035	24.954624
148.892738	5094.341818	24.959642
149.337423	5116.634707	24.964659
149.226308	5116.238600	24.969677
149.442042	5121.910314	24.974695
149.270053	5141.106411	24.979712
149.897791	5134.780589	24.984730
149.663921	5152.585612	24.989747
150.212088	5162.414230	24.994765
150.329203	5168.079026	24.999783
150.290751	5174.607798	25.004800
150.401465	5181.830499	25.009818
150.582156	5198.292148	25.014835
150.710245	5197.069037	25.019853
150.923658	5204.024754	25.024871
151.049810	5229.525471	25.029888
151.486857	5219.975287	25.034906
151.318964	5240.946596	25.039923
151.398521	5246.044734	25.044941
151.515757	5259.030754	25.049959
151.876787	5270.786618	25.054976
151.978081	5264.663096	25.059994
152.189286	5274.488401	25.065011
152.185365	5302.136537	25.070029
152.461474	5295.843158	25.075047
152.880273	5292.874190	25.080064
152.879003	5292.397324	25.085082
152.850143	5310.096597	25.090099
153.076460	5313.631369	25.095117
153.634482	5330.736004	25.100135
153.361963	5322.316889	25.105152
153.593273	5323.236783	25.110170
153.530429	5345.488255	25.115187
153.522325	5342.594935	25.120205
153.706116	5348.618504	25.125223
154.068640	5371.209221	25.130240
154.642098	5382.812340	25.135258
154.314258	5387.006472	25.140275
154.275765	5390.881900	25.145293
154.889634	5399.212247	25.150311
154.814590	5408.497073	25.155328
154.723949	5417.625803	25.160346
155.014296	5429.359603	25.165363
155.141434	5437.565252	25.170381
155.442968	5443.205976	25.175399
155.166925	5472.053443	25.180416
155.751175	5476.731611	25.185434
156.161491	5484.870414	25.190451
156.225171	5499.500319	25.195469
156.418574	5506.291348	25.200487
156.598381	5503.986707	25.205504
157.015233	5509.252847	25.210522
157.185183	5510.548289	25.215539
157.207449	5532.047294	25.220557
157.564724	5537.376837	25.225575
157.392278	5542.406854	25.230592
157.915174	5533.566005	25.235610
158.230313	5530.416460	25.240627
157.737030	5524.392656	25.245645
158.226957	5539.642408	25.250663
158.332507	5549.587324	25.255680
158.388245	5554.537511	25.260698
158.012091	5565.027047	25.265715
158.260331	5570.160418	25.270733
158.854931	5577.054500	25.275751
158.757031	5592.069107	25.280768
158.910196	5598.842806	25.285786
159.060619	5618.072445	25.290803
158.979091	5613.550451	25.295821
159.538478	5627.499676	25.300839
159.633482	5639.693524	25.305856
159.954518	5647.092739	25.310874
160.111966	5661.747858	25.315891
160.238349	5665.834724	25.320909
160.503388	5668.989904	25.325927
160.663687	5681.241508	25.330944
160.560828	5679.180029	25.335962
161.128069	5691.137600	25.340979
161.099409	5692.566674	25.345997
161.395469	5698.375346	25.351015
161.466223	5703.886952	25.356032
161.752664	5697.288518	25.361050
161.842844	5696.677616	25.366067
161.871976	5721.825038	25.371085
162.061393	5726.842574	25.376103
161.913619	5732.802557	25.381120
162.459607	5732.900695	25.386138
162.596995	5746.819741	25.391155
162.372350	5755.411680	25.396173
162.679205	5768.178972	25.401191
162.355584	5771.863779	25.406208
162.770384	5779.301508	25.411226
163.318446	5798.774370	25.416243
162.967388	5800.600077	25.421261
163.462876	5810.162969	25.426279
162.899059	5817.104450	25.431296
163.412805	5825.984321	25.436314
163.625487	5852.914080	25.441331
163.672723	5868.833840	25.446349
164.186675	5873.414282	25.451367
164.338234	5889.972824	25.456384
164.584310	5892.651587	25.461402
164.897161	5903.844548	25.466419
165.027836	5911.173359	25.471437
164.972032	5913.332632	25.476455
165.214071	5930.432253	25.481472
165.404849	5941.216608	25.486490
165.766205	5943.423904	25.491507
165.482745	5945.483376	25.496525
166.108479	5967.513674	25.501543
166.202967	5984.008506	25.506560
166.311089	5984.316812	25.511578
166.410162	5992.587635	25.516595
166.608540	6010.061541	25.521613
166.787483	6019.300430	25.526631
166.894070	6012.834747	25.531648
167.277666	6027.331958	25.536666
167.744831	6039.592203	25.541683
167.699300	6038.000410	25.546701
168.228067	6023.826016	25.551719
168.040019	6037.629382	25.556736
168.263990	6033.573009	25.561754
168.623850	6057.533869	25.566771
168.532352	6067.152956	25.571789
168.744916	6057.387352	25.576807
168.741282	6064.484450	25.581824
168.854729	6075.248600	25.586842
169.103962	6079.540508	25.591859
168.862603	6094.443451	25.596877
169.422660	6103.277633	25.601895
169.368202	6125.270517	25.606912
169.375217	6129.645775	25.611930
169.326710	6140.067379	25.616947
169.734259	6152.290311	25.621965
170.200821	6154.617678	25.626983
170.324755	6184.140638	25.632000
170.533971	6189.989831	25.637018
170.845072	6190.918252	25.642035
170.953407	6212.784345	25.647053
171.166591	6219.008544	25.652071
171.225735	6218.646097	25.657088
171.110851	6237.191080	25.662106
171.425182	6241.528978	25.667123
172.049071	6251.220557	25.672141
172.028155	6250.811485	25.677159
172.733808	6248.230056	25.682176
172.761066	6261.532613	25.687194
172.824054	6254.388881	25.692212
172.923688	6264.211193	25.697229
173.039011	6271.497425	25.702247
173.006979	6272.443958	25.707264
173.245637	6294.684760	25.712282
173.715402	6293.130655	25.717300
173.319287	6300.600635	25.722317
173.857650	6299.854230	25.727335
173.718241	6322.504054	25.732352
173.867888	6337.503278	25.737370
174.224069	6320.274721	25.742388
174.129414	6342.176109	25.747405
174.485721	6356.371782	25.752423
174.601634	6362.448304	25.757440
174.629441	6370.128635	25.762458
174.892332	6388.707456	25.767476
174.745037	6408.614136	25.772493
174.916722	6397.887978	25.777511
175.055381	6427.781469	25.782528
174.845538	6426.853118	25.787546
175.615246	6439.646468	25.792564
175.824035	6461.960958	25.797581
176.255679	6468.040481	25.802599
176.389003	6488.454538	25.807616
176.310254	6495.194884	25.812634
176.485080	6496.158441	25.817652
176.446711	6508.303335	25.822669
176.763670	6516.978671	25.827687
177.128147	6541.957016	25.832704
177.226399	6544.137386	25.837722
177.716262	6544.722062	25.842740
178.089912	6570.816465	25.847757
177.891693	6567.440063	25.852775
178.309408	6570.041756	25.857792
178.456676	6599.509663	25.862810
178.879781	6596.661421	25.867828
178.884927	6595.086400	25.872845
179.141034	6596.012120	25.877863
179.175490	6612.780573	25.882880
179.300641	6626.260212	25.887898
179.658156	6620.760096	25.892916
179.749223	6635.745658	25.897933
179.838383	6651.704175	25.902951
180.080763	6669.277076	25.907968
180.187684	6661.998318	25.912986
180.474054	6673.599038	25.918004
180.272743	6697.258245	25.923021
180.441231	6700.007459	25.928039
181.064433	6716.378688	25.933056
181.028846	6733.727457	25.938074
181.803186	6728.847544	25.943092
181.642177	6737.747674	25.948109
181.774967	6748.279910	25.953127
181.843615	6767.055872	25.958144
181.806223	6763.345707	25.963162
182.107783	6769.660269	25.968180
182.193290	6797.223411	25.973197
182.489072	6793.610976	25.978215
182.870059	6807.007546	25.983232
182.799946	6831.159553	25.988250
182.661133	6833.892623	25.993268
182.898024	6860.109335	25.998285
183.402689	6852.663963	26.003303
183.753012	6860.788197	26.008320
183.660326	6886.884571	26.013338
184.182926	6879.574834	26.018356
184.219644	6908.407120	26.023373
184.197278	6916.900112	26.028391
184.805056	6910.515064	26.033408
184.679343	6928.687768	26.038426
185.235967	6933.862387	26.043444
185.270489	6938.876765	26.048461
185.576899	6942.642034	26.053479
186.008731	6943.683653	26.058496
185.925038	6970.524504	26.063514
186.307536	6968.551593	26.068532
186.606803	6968.292005	26.073549
186.495570	6975.382090	26.078567
186.631710	6973.338049	26.083584
186.381365	6967.806724	26.088602
186.631260	6976.564277	26.093620
186.684219	6991.968373	26.098637
186.766665	6989.363789	26.103655
187.105795	7013.179896	26.108672
187.201135	7031.278390	26.113690
187.609748	7035.889184	26.118708
187.482242	7056.934602	26.123725
187.762713	7056.414281	26.128743
188.295345	7075.919635	26.133760
188.255196	7101.297292	26.138778
188.343778	7096.101347	26.143796
188.658234	7114.352751	26.148813
188.921485	7119.487698	26.153831
188.946811	7129.174763	26.158848
188.886120	7147.829210	26.163866
189.106721	7157.543096	26.168884
189.590471	7178.941325	26.173901
189.451191	7192.592728	26.178919
190.213561	7208.143659	26.183936
189.937593	7236.317812	26.188954
189.986291	7235.663301	26.193972
190.396196	7255.892465	26.198989
190.442943	7273.525143	26.204007
191.160486	7276.839797	26.209024
190.767045	7297.601840	26.214042
191.335569	7303.621269	26.219060
191.353504	7312.530748	26.224077
191.785461	7341.671049	26.229095
192.189124	7339.107845	26.234112
192.397562	7354.482667	26.239130
192.294853	7367.494171	26.244148
192.863226	7369.278795	26.249165
192.704146	7376.517156	26.254183
193.008480	7395.906261	26.259200
193.284976	7402.700923	26.264218
193.425686	7404.120676	26.269236
193.794479	7425.972984	26.274253
193.848853	7427.739367	26.279271
194.100573	7442.531395	26.284288
194.566160	7458.415145	26.289306
194.684532	7471.646961	26.294324
194.667503	7472.691111	26.299341
194.521704	7474.815061	26.304359
195.126499	7496.322100	26.309376
195.259846	7501.715701	26.314394
195.257788	7521.755730	26.319412
195.889832	7528.807527	26.324429
195.635598	7537.929072	26.329447
195.767169	7546.652936	26.334464
196.081369	7562.439727	26.339482
196.288977	7576.364936	26.344500
196.531667	7583.127458	26.349517
196.767969	7600.527556	26.354535
196.763373	7602.056396	26.359552
196.982092	7618.470983	26.364570
197.064568	7621.415719	26.369588
197.505590	7647.064445	26.374605
197.447092	7656.165531	26.379623
198.003294	7667.633403	26.384640
198.184098	7688.318405	26.389658
198.335458	7684.309840	26.394676
198.605366	7703.973584	26.399693
198.836556	7724.651883	26.404711
199.065220	7725.843693	26.409728
199.068783	7739.442824	26.414746
199.345141	7744.385209	26.419764
199.777476	7747.593507	26.424781
199.597338	7762.774595	26.429799
200.046570	7767.851459	26.434816
199.801565	7785.657354	26.439834
200.187152	7798.213632	26.444852
200.286358	7793.221269	26.449869
200.171881	7816.071530	26.454887
200.688043	7826.577374	26.459904
200.787053	7842.961566	26.464922
201.082652	7852.611508	26.469940
201.353180	7864.316538	26.474957
201.235036	7887.132853	26.479975
201.663926	7891.256956	26.484992
201.892894	7905.567220	26.490010
202.255230	7919.663284	26.495028
202.471166	7925.294633	26.500045
202.667233	7943.783153	26.505063
203.052168	7945.839953	26.510080
203.016721	7962.012562	26.515098
203.041396	7969.816271	26.520116
203.303939	7978.931446	26.525133
203.532816	7989.391927	26.530151
203.784587	7997.102994	26.535168
204.062495	8016.318438	26.540186
204.176436	8035.156159	26.545204
204.751268	8042.546080	26.550221
204.581930	8060.041273	26.555239
204.958465	8058.062916	26.560256
205.133389	8081.762057	26.565274
205.186009	8089.865230	26.570292
205.867424	8092.279478	26.575309
205.886897	8110.519339	26.580327
205.832137	8112.994577	26.585344
206.608799	8124.732744	26.590362
206.490769	8143.858599	26.595380
206.778442	8151.798523	26.600397
206.965378	8161.611531	26.605415
207.361779	8156.211580	26.610432
207.457403	8176.455259	26.615450
207.609522	8184.403418	26.620468
207.852072	8189.965880	26.625485
208.002710	8204.950965	26.630503
207.993683	8216.067618	26.635520
208.399298	8216.673375	26.640538
208.504120	8235.119026	26.645556
208.791397	8242.706203	26.650573
208.720333	8255.509211	26.655591
208.935152	8262.047429	26.660608
209.120541	8282.033821	26.665626
208.953610	8308.492152	26.670644
209.449774	8311.010293	26.675661
209.904092	8337.006865	26.680679
210.026809	8341.436081	26.685696
210.361584	8361.545180	26.690714
210.583334	8382.019538	26.695732
210.917574	8392.880327	26.700749
210.801986	8413.252146	26.705767
210.741771	8412.809341	26.710784
211.082288	8443.705892	26.715802
211.267463	8446.451869	26.720820
212.094337	8467.914091	26.725837
211.979330	8481.175860	26.730855
212.140983	8490.656926	26.735872
212.270711	8510.018749	26.740890
212.486127	8513.582830	26.745908
212.798355	8532.247393	26.750925
212.781755	8549.087772	26.755943
213.183878	8555.323427	26.760960
213.765766	8565.167523	26.765978
213.498284	8557.268441	26.770996
213.489632	8584.106717	26.776013
213.950890	8599.926171	26.781031
214.297498	8608.028294	26.786048
214.665209	8626.160802	26.791066
214.725590	8631.773209	26.796084
215.370670	8642.504834	26.801101
215.066551	8660.407330	26.806119
215.616874	8667.937072	26.811136
215.684786	8678.430118	26.816154
215.396095	8691.641994	26.821172
216.047406	8701.719666	26.826189
215.788389	8724.591965	26.831207
216.044291	8731.503239	26.836224
216.516789	8756.655494	26.841242
216.245371	8767.650477	26.846260
216.721344	8787.857299	26.851277
216.992913	8809.844947	26.856295
217.261420	8828.803791	26.861312
217.404944	8840.207588	26.866330
217.562696	8868.702081	26.871348
218.297228	8877.278223	26.876365
218.304908	8906.044904	26.881383
218.302246	8915.343066	26.886400
218.751496	8918.711072	26.891418
218.528688	8944.212440	26.896436
219.289988	8955.998665	26.901453
219.218638	8964.118041	26.906471
219.392370	8993.958604	26.911488
219.638194	9007.204516	26.916506
219.507634	9025.338676	26.921524
220.271132	9044.183699	26.926541
220.593495	9057.895911	26.931559
220.720935	9074.985582	26.936576
220.962551	9089.179827	26.941594
221.030096	9102.629350	26.946612
221.531694	9120.926194	26.951629
221.858625	9138.583182	26.956647
221.665692	9151.553553	26.961664
221.803757	9167.400980	26.966682
222.087302	9191.219312	26.971700
222.866437	9196.613130	26.976717
223.020600	9224.006104	26.981735
222.976686	9232.879620	26.986752
223.672439	9232.845936	26.991770
223.296052	9262.635324	26.996788
223.502141	9258.949723	27.001805
224.330320	9286.355109	27.006823
224.158669	9288.959329	27.011840
224.462437	9306.580159	27.016858
224.495100	9318.418514	27.021876
225.328207	9330.218361	27.026893
225.584759	9350.702398	27.031911
225.492236	9358.633278	27.036928
225.974431	9349.010935	27.041946
225.928237	9373.155771	27.046964
226.234382	9383.667423	27.051981
226.439219	9397.059066	27.056999
226.428437	9398.055835	27.062016
226.667593	9404.490469	27.067034
227.003286	9429.809754	27.072052
227.689593	9428.941107	27.077069
227.712731	9449.781275	27.082087
227.947384	9456.174139	27.087104
228.334873	9471.061423	27.092122
228.242310	9488.474607	27.097140
228.968160	9489.034600	27.102157
228.957104	9507.537108	27.107175
228.788607	9511.743800	27.112192
229.282148	9507.943694	27.117210
229.114280	9527.170031	27.122228
229.092642	9535.350801	27.127245
229.489052	9543.434149	27.132263
229.248258	9569.013531	27.137280
229.761831	9564.253840	27.142298
229.612090	9598.660118	27.147316
230.070697	9615.051317	27.152333
230.329705	9640.450562	27.157351
230.100239	9657.488761	27.162368
230.649491	9682.211533	27.167386
230.957444	9705.170371	27.172404
231.214765	9724.503928	27.177421
231.732388	9746.201728	27.182439
231.952937	9767.901377	27.187456
232.419843	9774.284354	27.192474
232.480444	9792.830493	27.197492
232.929553	9797.908826	27.202509
233.052221	9808.187978	27.207527
233.102387	9832.643701	27.212544
233.625569	9840.017009	27.217562
233.722844	9871.522101	27.222580
234.014977	9872.616943	27.227597
234.427017	9903.836931	27.232615
234.471563	9914.126696	27.237632
234.854029	9921.153854	27.242650
234.762208	9939.355909	27.247668
234.955823	9946.125976	27.252685
235.199410	9966.790184	27.257703
235.308313	9986.748033	27.262720
235.679960	10007.295821	27.267738
236.045106	10034.181123	27.272756
236.207051	10043.736326	27.277773
236.573230	10055.321619	27.282791
236.845024	10068.712217	27.287808
237.270702	10090.620245	27.292826
237.151832	10103.641382	27.297844
237.571410	10119.938723	27.302861
237.928772	10138.977400	27.307879
238.028845	10146.119846	27.312896
238.482756	10156.884088	27.317914
238.853709	10173.223389	27.322932
238.826560	10195.504138	27.327949
239.157281	10202.360368	27.332967
239.340823	10219.449088	27.337984
239.693530	10224.301653	27.343002
239.693068	10247.198795	27.348020
240.141386	10267.242708	27.353037
240.220755	10276.205928	27.358055
240.140936	10296.346589	27.363072
240.777854	10321.512755	27.368090
241.001529	10333.863052	27.373108
240.927853	10335.589473	27.378125
241.215679	10352.176649	27.383143
241.560693	10368.530676	27.388160
241.874014	10382.910375	27.393178
242.387500	10410.288558	27.398196
242.633108	10422.477753	27.403213
243.229899	10425.872912	27.408231
243.325842	10440.077463	27.413248
243.560215	10436.544468	27.418266
243.707857	10459.634860	27.423284
244.213116	10472.171125	27.428301
244.074490	10470.391029	27.433319
243.870529	10486.776798	27.438336
244.439371	10489.395148	27.443354
244.369862	10508.127465	27.448372
244.593731	10521.789467	27.453389
245.061225	10550.179074	27.458407
245.097916	10562.150027	27.463424
245.508024	10571.422708	27.468442
245.444966	10590.124120	27.473460
245.751881	10597.127036	27.478477
246.323967	10620.878565	27.483495
246.063860	10635.909383	27.488512
246.475360	10644.514653	27.493530
246.624946	10678.081321	27.498548
247.080963	10691.280516	27.503565
247.606438	10703.874281	27.508583
246.914092	10725.577962	27.513600
247.556649	10743.358677	27.518618
248.019809	10766.665219	27.523636
247.855133	10802.273940	27.528653
248.615905	10805.641302	27.533671
248.780651	10845.156535	27.538688
248.618832	10848.159564	27.543706
248.975633	10866.168812	27.548724
249.606608	10893.362983	27.553741
250.051029	10896.509278	27.558759
249.860047	10921.493343	27.563776
250.700081	10938.968297	27.568794
250.614522	10959.651144	27.573812
250.897618	10975.601660	27.578829
251.340675	10980.820021	27.583847
251.546198	11011.271985	27.588864
251.743888	11031.387414	27.593882
251.859865	11040.325320	27.598900
252.229758	11071.576612	27.603917
252.632309	11069.161900	27.608935
252.935604	11097.486650	27.613952
252.997204	11100.634788	27.618970
253.336208	11116.231163	27.623988
253.258841	11131.527667	27.629005
253.572325	11154.321455	27.634023
253.770004	11174.296840	27.639040
253.978304	11186.968599	27.644058
254.320467	11206.247393	27.649076
254.478638	11231.611471	27.654093
255.167502	11255.954391	27.659111
255.160857	11266.336200	27.664128
255.627983	11297.086595	27.669146
255.804364	11303.169202	27.674164
255.767850	11332.609288	27.679181
256.415213	11336.929814	27.684199
256.898718	11363.318038	27.689216
257.493965	11364.976593	27.694234
257.324859	11384.919093	27.699252
257.441601	11396.538695	27.704269
257.480619	11408.184538	27.709287
257.489461	11418.745078	27.714304
258.249108	11452.638770	27.719322
258.605754	11456.218783	27.724340
258.627159	11482.570107	27.729357
258.896061	11506.948919	27.734375
259.090284	11514.280460	27.739392
259.298666	11529.712900	27.744410
259.634594	11560.691878	27.749428
259.580680	11570.644467	27.754445
260.264892	11585.774613	27.759463
260.638453	11606.705436	27.764480
260.716425	11638.091144	27.769498
261.195915	11646.617184	27.774516
261.225040	11676.609544	27.779533
261.769744	11661.415207	27.784551
262.409652	11679.943451	27.789568
262.467729	11699.298922	27.794586
262.628623	11702.017966	27.799604
262.517029	11706.864976	27.804621
262.968972	11718.955683	27.809639
263.183883	11727.378160	27.814656
263.553298	11738.625387	27.819674
263.921390	11743.571201	27.824692
263.640666	11762.480892	27.829709
264.115009	11778.180814	27.834727
264.088603	11793.741320	27.839744
264.283174	11826.115734	27.844762
264.928243	11831.726417	27.849780
264.809814	11859.866151	27.854797
265.434553	11882.224312	27.859815
265.437736	11907.909705	27.864832
265.684181	11922.877728	27.869850
265.910100	11940.828664	27.874868
265.964714	11975.018776	27.879885
266.244984	11986.986000	27.884903
266.163807	12020.349377	27.889920
267.068996	12038.441874	27.894938
267.629118	12051.837706	27.899956
267.960930	12074.223259	27.904973
268.547048	12089.295246	27.909991
268.600810	12109.280603	27.915008
268.716257	12111.052386	27.920026
269.220140	12136.815349	27.925044
269.594585	12152.923690	27.930061
269.733623	12166.560932	27.935079
270.037622	12176.614692	27.940096
270.138805	12186.579065	27.945114
270.512482	12192.831885	27.950132
270.451835	12211.861732	27.955149
270.468327	12231.123084	27.960167
270.669244	12262.362856	27.965184
270.440172	12284.954027	27.970202
271.048163	12304.922117	27.975220
271.217358	12339.331208	27.980237
271.579706	12356.681012	27.985255
271.931199	12390.637816	27.990272
272.565794	12412.004778	27.995290
272.862361	12447.705592	28.000308
273.119428	12471.841229	28.005325
273.411864	12480.250506	28.010343
273.817933	12508.850690	28.015360
273.909799	12524.309637	28.020378
273.919822	12539.633219	28.025396
273.835561	12579.582260	28.030413
274.551800	12593.568058	28.035431
274.686990	12624.068574	28.040448
275.213694	12648.994258	28.045466
275.575258	12671.059011	28.050484
275.666335	12694.744181	28.055501
276.583539	12722.671775	28.060519
276.878510	12734.440951	28.065536
276.677409	12759.216027	28.070554
276.954472	12769.678777	28.075572
277.186279	12786.242273	28.080589
277.276299	12800.345893	28.085607
277.934157	12826.759714	28.090624
278.219223	12849.226550	28.095642
279.104280	12865.489966	28.100660
278.943574	12882.739242	28.105677
278.801236	12892.611136	28.110695
279.395848	12912.926487	28.115712
279.539076	12932.531728	28.120730
280.030615	12950.366635	28.125748
280.041286	12961.354116	28.130765
280.396866	12987.230395	28.135783
280.735261	13010.068394	28.140800
280.629870	13026.267126	28.145818
281.123212	13046.010053	28.150836
281.427129	13061.652720	28.155853
281.991622	13079.844440	28.160871
281.802888	13101.849427	28.165888
281.758689	13116.884699	28.170906
282.264407	13141.847703	28.175924
282.380817	13172.692718	28.180941
282.966213	13189.256513	28.185959
283.468072	13209.365382	28.190976
283.403746	13246.428366	28.195994
284.146788	13255.177239	28.201012
284.364269	13287.231710	28.206029
284.543195	13306.762174	28.211047
284.975805	13306.695568	28.216064
285.011914	13333.625789	28.221082
285.378396	13339.485518	28.226100
285.451057	13360.086212	28.231117
286.108676	13391.866477	28.236135
286.140602	13405.961313	28.241152
286.275744	13429.838827	28.246170
286.994009	13448.985688	28.251188
287.000876	13467.975918	28.256205
287.399396	13498.319547	28.261223
288.228572	13520.713182	28.266240
288.031604	13535.052373	28.271258
288.922656	13564.043098	28.276276
288.831951	13569.168491	28.281293
289.243306	13589.021750	28.286311
289.464710	13612.585882	28.291328
289.570661	13624.773005	28.296346
289.817345	13649.021634	28.301364
290.047425	13663.436935	28.306381
290.261309	13685.934028	28.311399
290.631410	13711.894161	28.316416
290.954130	13733.906903	28.321434
291.259007	13756.592339	28.326452
291.396355	13777.453914	28.331469
291.979640	13790.553483	28.336487
292.655496	13805.927417	28.341504
292.890755	13836.148950	28.346522
293.361645	13834.200806	28.351540
293.077477	13853.783224	28.356557
293.592515	13878.419634	28.361575
294.131643	13886.531245	28.366592
294.176097	13909.450594	28.371610
294.311859	13930.003767	28.376628
294.534872	13951.940305	28.381645
294.735593	13967.545745	28.386663
295.038096	13990.003406	28.391680
295.242972	14010.819457	28.396698
295.910117	14033.500585	28.401716
295.763422	14060.176987	28.406733
296.156451	14072.670006	28.411751
296.950743	14095.254575	28.416768
296.995536	14116.384011	28.421786
297.040978	14136.369307	28.426804
297.353366	14157.118932	28.431821
297.614081	14189.848809	28.436839
297.687839	14198.729257	28.441856
297.873460	14229.230767	28.446874
298.522749	14257.249407	28.451892
298.946755	14280.502113	28.456909
299.463496	14306.582375	28.461927
300.049552	14325.435373	28.466944
300.222686	14336.510407	28.471962
300.876403	14343.133041	28.476980
301.097342	14359.438351	28.481997
301.060401	14373.217626	28.487015
301.584104	14378.052664	28.492032
301.334561	14392.609310	28.497050
301.665026	14405.158622	28.502068
301.996470	14432.842414	28.507085
302.217121	14431.368907	28.512103
302.286552	14461.671004	28.517120
301.986444	14491.958566	28.522138
302.518996	14499.370309	28.527156
302.684927	14545.971659	28.532173
303.023853	14583.256307	28.537191
303.834343	14600.525029	28.542208
304.061012	14640.594032	28.547226
304.380032	14661.702509	28.552244
304.851381	14682.757482	28.557261
305.171681	14723.821367	28.562279
305.597328	14719.846115	28.567296
305.833543	14749.448285	28.572314
306.118701	14785.434282	28.577332
306.045445	14800.543676	28.582349
306.119365	14831.236542	28.587367
306.622630	14857.955007	28.592384
306.827325	14888.656319	28.597402
307.248553	14920.466030	28.602420
307.848799	14941.031996	28.607437
307.807555	14970.278546	28.612455
308.408669	15001.997238	28.617472
308.526212	15036.911487	28.622490
308.767757	15059.883418	28.627508
309.103702	15092.916293	28.632525
309.652489	15112.359458	28.637543
310.202214	15134.379147	28.642560
310.132417	15170.612172	28.647578
310.616129	15194.215635	28.652596
311.113299	15223.956789	28.657613
311.449997	15253.779667	28.662631
312.129970	15273.105219	28.667648
311.907908	15291.705163	28.672666
312.387928	15308.126217	28.677684
312.632832	15343.436133	28.682701
313.163358	15363.399529	28.687719
313.186232	15375.559138	28.692736
313.762258	15416.875650	28.697754
314.111934	15430.078181	28.702772
314.367845	15455.587176	28.707789
314.444735	15483.866397	28.712807
315.160114	15507.895377	28.717824
315.140550	15528.581819	28.722842
315.495693	15553.002910	28.727860
315.734734	15575.151745	28.732877
316.037830	15595.493410	28.737895
316.319552	15609.547311	28.742912
316.571839	15640.552643	28.747930
317.067634	15672.406662	28.752948
317.428117	15695.615150	28.757965
317.627657	15727.437844	28.762983
318.269321	15740.762596	28.768000
318.521062	15773.399424	28.773018
318.706939	15789.328991	28.778036
318.973848	15803.620330	28.783053
319.061702	15837.184258	28.788071
319.477080	15858.729104	28.793088
319.673021	15889.457384	28.798106
320.191634	15923.829738	28.803124
320.522322	15938.336028	28.808141
320.926689	15974.651676	28.813159
321.287381	15985.411587	28.818176
321.501606	16008.416159	28.823194
321.813141	16023.020249	28.828212
322.141501	16050.007544	28.833229
322.296484	16074.237110	28.838247
322.871543	16092.777195	28.843264
322.961219	16124.864672	28.848282
323.452412	16144.383203	28.853300
323.628505	16166.834805	28.858317
323.668400	16209.942436	28.863335
324.138728	16223.841200	28.868352
324.462279	16245.976982	28.873370
324.513139	16277.905687	28.878388
324.817464	16304.880036	28.883405
325.002585	16342.263455	28.888423
325.544774	16367.310500	28.893440
325.752583	16407.557164	28.898458
326.102611	16440.084520	28.903476
327.068014	16476.603319	28.908493
327.214367	16498.414102	28.913511
327.628198	16521.696904	28.918528
327.601432	16552.655500	28.923546
327.674436	16575.646373	28.928564
328.595137	16613.265082	28.933581
328.649501	16651.553411	28.938599
329.122190	16666.531778	28.943616
329.388128	16700.540877	28.948634
330.077215	16731.104156	28.953652
330.722810	16748.775941	28.958669
330.494589	16781.944831	28.963687
330.734039	16810.221550	28.968704
331.375672	16829.744415	28.973722
331.472236	16863.550146	28.978740
332.158162	16888.047823	28.983757
332.046750	16915.883063	28.988775
332.444509	16941.320503	28.993792
333.040781	16977.959719	28.998810
333.291709	17001.156634	29.003828
334.225472	17020.633042	29.008845
334.319993	17035.639547	29.013863
334.246640	17067.500467	29.018880
334.924973	17085.460366	29.023898
335.147326	17102.731194	29.028916
335.531396	17131.659156	29.033933
336.103715	17169.127071	29.038951
335.908255	17185.094198	29.043968
336.244513	17208.471173	29.048986
336.721774	17236.854344	29.054004
337.237144	17253.528426	29.059021
337.290880	17280.148589	29.064039
337.720684	17302.284005	29.069056
338.202040	17341.250492	29.074074
338.335763	17369.109045	29.079092
338.711096	17387.311622	29.084109
339.015930	17423.467239	29.089127
338.828288	17452.518585	29.094144
339.365065	17493.827906	29.099162
339.591944	17533.979606	29.104180
340.066896	17553.409506	29.109197
340.457455	17587.708780	29.114215
340.986205	17624.086338	29.119232
340.986761	17648.651091	29.124250
341.077259	17687.181742	29.129268
341.887366	17712.831239	29.134285
341.966992	17742.743671	29.139303
342.644157	17779.144338	29.144320
343.176967	17810.022311	29.149338
343.439992	17832.017339	29.154356
343.919155	17860.109675	29.159373
344.345368	17871.569292	29.164391
344.555904	17894.618095	29.169408
345.136926	17921.185283	29.174426
345.149897	17933.493433	29.179444
345.689465	17960.058075	29.184461
345.834910	17982.952253	29.189479
345.817934	18007.388034	29.194496
346.650045	18032.821608	29.199514
346.717400	18076.054109	29.204532
347.275483	18085.443006	29.209549
347.371388	18119.784184	29.214567
347.516158	18152.334649	29.219584
348.056000	18174.979520	29.224602
348.018401	18210.523536	29.229620
348.691287	18237.462235	29.234637
348.708857	18276.529618	29.239655
349.127917	18313.071830	29.244672
349.926922	18347.771777	29.249690
350.204352	18376.730576	29.254708
350.697683	18402.088283	29.259725
350.742138	18443.418265	29.264743
350.775225	18463.609481	29.269760
351.399487	18495.986835	29.274778
351.685289	18534.484044	29.279796
352.065459	18562.349608	29.284813
352.390959	18598.562706	29.289831
352.707756	18637.412847	29.294848
353.247424	18658.270919	29.299866
353.694768	18707.923933	29.304884
354.827132	18729.254794	29.309901
355.228072	18752.516086	29.314919
355.314755	18774.943454	29.319936
356.112981	18794.885724	29.324954
356.399400	18814.237916	29.329972
356.582004	18830.238750	29.334989
356.970611	18864.520507	29.340007
356.842680	18885.074588	29.345024
357.533355	18911.332066	29.350042
357.455949	18940.530168	29.355060
358.080061	18968.218979	29.360077
358.134926	18994.260059	29.365095
357.940216	19025.358221	29.370112
358.584354	19060.752029	29.375130
359.224679	19093.134204	29.380148
359.734060	19117.713234	29.385165
359.944471	19161.763535	29.390183
360.187845	19189.118381	29.395200
360.771292	19219.292312	29.400218
360.794286	19259.097257	29.405236
361.256472	19284.217131	29.410253
361.726360	19333.475788	29.415271
361.661160	19356.966263	29.420288
362.316912	19391.890687	29.425306
362.395026	19437.379130	29.430324
363.037030	19461.485926	29.435341
363.420990	19509.547087	29.440359
363.606189	19550.722584	29.445376
364.495745	19571.902334	29.450394
364.420206	19619.049766	29.455412
364.975093	19638.967048	29.460429
365.470243	19658.440228	29.465447
365.841563	19704.082738	29.470464
366.004173	19729.612188	29.475482
366.417581	19757.844720	29.480500
367.037607	19788.100344	29.485517
367.058567	19820.280440	29.490535
367.191313	19843.902846	29.495552
367.683334	19871.004926	29.500570
367.837982	19912.599379	29.505588
368.082248	19944.856326	29.510605
368.788588	19978.946020	29.515623
368.983741	20013.842224	29.520640
369.499822	20045.583119	29.525658
369.493438	20082.104927	29.530676
370.199161	20114.739977	29.535693
370.761706	20151.859998	29.540711
370.838377	20186.115617	29.545728
371.529122	20218.274114	29.550746
371.629648	20245.640107	29.555764
372.143410	20283.304464	29.560781
372.548127	20311.621346	29.565799
372.790588	20351.900258	29.570816
373.211883	20384.355817	29.575834
373.430854	20415.785495	29.580852
373.809055	20459.504105	29.585869
374.135166	20499.337608	29.590887
374.431591	20540.987452	29.595904
375.349436	20579.984039	29.600922
375.607693	20615.840598	29.605940
375.789341	20647.234313	29.610957
376.354736	20681.504800	29.615975
376.419526	20715.861209	29.620992
377.050572	20746.105719	29.626010
377.286619	20783.005200	29.631028
377.831399	20821.341955	29.636045
378.456486	20847.195566	29.641063
378.348404	20893.924747	29.646080
379.033026	20918.783330	29.651098
379.066642	20968.081055	29.656116
379.864724	20998.331536	29.661133
379.972249	21032.528615	29.666151
380.322514	21085.184341	29.671168
380.939060	21118.238097	29.676186
381.257516	21157.863182	29.681204
381.697527	21190.293569	29.686221
382.079565	21217.037644	29.691239
382.296261	21266.321767	29.696256
382.702150	21292.423532	29.701274
383.013055	21336.459821	29.706292
383.549479	21365.105145	29.711309
383.615263	21400.359839	29.716327
384.251785	21455.763057	29.721344
384.702802	21486.558907	29.726362
385.238283	21535.986652	29.731380
385.575779	21563.563172	29.736397
385.826213	21583.961898	29.741415
386.203002	21640.256817	29.746432
386.620336	21673.333543	29.751450
386.876610	21721.337030	29.756468
387.293053	21758.964033	29.761485
388.160683	21795.017269	29.766503
388.208045	21840.760123	29.771520
388.621478	21879.914018	29.776538
388.872750	21913.598831	29.781556
389.307907	21955.975000	29.786573
390.065559	21978.332094	29.791591
390.391198	22017.494507	29.796608
390.817208	22041.919777	29.801626
391.193517	22078.016947	29.806644
391.442995	22119.702121	29.811661
391.896335	22143.492384	29.816679
392.229481	22182.958227	29.821696
392.723522	22224.224875	29.826714
393.002003	22251.228929	29.831732
393.248184	22290.398797	29.836749
393.765528	22312.512244	29.841767
393.718064	22348.446660	29.846784
394.446505	22383.436287	29.851802
395.204792	22409.825282	29.856820
395.239440	22444.619051	29.861837
395.932078	22470.711544	29.866855
396.309735	22509.421899	29.871872
396.727817	22538.367842	29.876890
396.890528	22569.872342	29.881908
396.964843	22592.850817	29.886925
397.596295	22629.000045	29.891943
397.961220	22678.853490	29.896960
398.502417	22703.221278	29.901978
398.519013	22744.102958	29.906996
398.756681	22789.151600	29.912013
399.533808	22826.037138	29.917031
399.436283	22878.980578	29.922048
399.838383	22912.328717	29.927066
400.171117	22962.517843	29.932084
400.200539	22999.956134	29.937101
401.012222	23053.408979	29.942119
401.358637	23112.933437	29.947136
401.851014	23158.685188	29.952154
402.124979	23207.905623	29.957172
402.521955	23256.542996	29.962189
403.292561	23294.064472	29.967207
403.587445	23344.371355	29.972224
403.904833	23386.806843	29.977242
404.809918	23434.521980	29.982260
404.932799	23477.940591	29.987277
405.618103	23520.165848	29.992295
405.865153	23564.128639	29.997312
406.335788	23600.470496	30.002330
406.861526	23636.312963	30.007348
407.398855	23690.251479	30.012365
407.877193	23725.643132	30.017383
408.014871	23768.072998	30.022400
408.166614	23808.220655	30.027418
408.890236	23861.167120	30.032436
409.165470	23888.817650	30.037453
410.354776	23920.721142	30.042471
410.424719	23954.171933	30.047488
410.879442	23990.340658	30.052506
411.274891	24028.212712	30.057524
411.053118	24085.198077	30.062541
411.737303	24116.847949	30.067559
412.341561	24168.544204	30.072576
412.314002	24201.659965	30.077594
413.193607	24255.113275	30.082612
413.586547	24299.355042	30.087629
414.204148	24324.450494	30.092647
414.355380	24380.252545	30.097664
414.884079	24410.050670	30.102682
415.360808	24447.754129	30.107700
415.512299	24484.937436	30.112717
415.686741	24529.081865	30.117735
416.253930	24577.802139	30.122752
416.616535	24617.167882	30.127770
417.403131	24649.594980	30.132788
417.698039	24701.348691	30.137805
418.482329	24737.117663	30.142823
418.289116	24778.482000	30.147840
418.805620	24838.290328	30.152858
419.213180	24869.197299	30.157876
419.395647	24917.340317	30.162893
419.703110	24955.194282	30.167911
420.152433	24997.347092	30.172928
420.716629	25037.353830	30.177946
420.780843	25074.857179	30.182964
421.717328	25117.839670	30.187981
421.967402	25152.303802	30.192999
422.345385	25198.294411	30.198016
422.581846	25243.471193	30.203034
422.883884	25286.836448	30.208052
423.553701	25332.337680	30.213069
423.955412	25368.447137	30.218087
424.624366	25418.780372	30.223104
424.886708	25459.610650	30.228122
425.414265	25504.945037	30.233140
425.560791	25552.386174	30.238157
426.033235	25594.073026	30.243175
426.829794	25642.338997	30.248192
426.885633	25695.256411	30.253210
427.421818	25720.491955	30.258228
427.715542	25781.745443	30.263245
428.292224	25825.744784	30.268263
428.616182	25874.614602	30.273280
429.084465	25929.658147	30.278298
429.443315	25974.759876	30.283316
429.546161	26028.419611	30.288333
430.157843	26073.451450	30.293351
430.529834	26125.833842	30.298368
431.085392	26179.785127	30.303386
431.837811	26232.120772	30.308404
432.264890	26284.040378	30.313421
432.668157	26332.542005	30.318439
433.058023	26371.602935	30.323456
433.126846	26416.365795	30.328474
434.192905	26470.075967	30.333492
433.998381	26518.998577	30.338509
434.565101	26575.248541	30.343527
434.764587	26626.743139	30.348544
434.985959	26687.456708	30.353562
435.853455	26746.496193	30.358580
436.387729	26802.181377	30.363597
436.500197	26864.619913	30.368615
437.171845	26915.911220	30.373632
437.376185	26976.209129	30.378650
438.040459	27024.445655	30.383668
438.273863	27081.010974	30.388685
438.908754	27137.469155	30.393703
439.217433	27190.174360	30.398720
439.860644	27251.624545	30.403738
440.419506	27299.343051	30.408756
440.555924	27355.887444	30.413773
441.477993	27411.933205	30.418791
441.581099	27459.617044	30.423808
442.079138	27524.653264	30.428826
442.987517	27554.755317	30.433844
443.229777	27610.229557	30.438861
443.711105	27651.334840	30.443879
444.603068	27705.203807	30.448896
444.682652	27751.586486	30.453914
445.252297	27801.704983	30.458932
445.254003	27851.091024	30.463949
446.194458	27899.795376	30.468967
446.618361	27958.508555	30.473984
446.571245	28010.057488	30.479002
447.163556	28044.716936	30.484020
447.602489	28106.412099	30.489037
447.868999	28167.858384	30.494055
448.850720	28206.362033	30.499072
449.177547	28261.029506	30.504090
449.550417	28298.716022	30.509108
449.927993	28343.029132	30.514125
450.502245	28382.679271	30.519143
451.246550	28427.297925	30.524160
451.181753	28474.447670	30.529178
451.949809	28507.716329	30.534196
452.445148	28554.023022	30.539213
452.749241	28593.566860	30.544231
453.311058	28636.878737	30.549248
453.729827	28693.005494	30.554266
454.350327	28726.261095	30.559284
454.310829	28767.546548	30.564301
454.908468	28815.130357	30.569319
455.578337	28863.800113	30.574336
455.507535	28918.447020	30.579354
456.316930	28957.248941	30.584372
456.562147	29007.796754	30.589389
456.745436	29063.086665	30.594407
457.233460	29108.664211	30.599424
457.417926	29169.689130	30.604442
458.073068	29215.737764	30.609460
458.181853	29288.586087	30.614477
458.916133	29344.451484	30.619495
459.472382	29406.150828	30.624512
459.814331	29459.056193	30.629530
460.477379	29520.653130	30.634548
461.030039	29574.681767	30.639565
461.271370	29630.490710	30.644583
462.191377	29687.288680	30.649600
462.190586	29741.582759	30.654618
463.044008	29793.546604	30.659636
463.359308	29856.290514	30.664653
463.400556	29911.991452	30.669671
464.458485	29973.051569	30.674688
465.062083	30029.262529	30.679706
465.267338	30083.277575	30.684724
465.606824	30137.696496	30.689741
466.241702	30193.546341	30.694759
466.949023	30246.008875	30.699776
467.408626	30303.506385	30.704794
467.696371	30351.871178	30.709812
468.211537	30417.641013	30.714829
468.303163	30478.433477	30.719847
468.934441	30524.558925	30.724864
469.050005	30592.591130	30.729882
470.082178	30646.666922	30.734900
470.942937	30711.891793	30.739917
471.270331	30765.295675	30.744935
471.846959	30816.182035	30.749952
472.368462	30863.894448	30.754970
472.901150	30914.018578	30.759988
473.717218	30974.197797	30.765005
474.004525	31025.643639	30.770023
474.276405	31059.033855	30.775040
474.442679	31119.664785	30.780058
474.935404	31172.443179	30.785076
475.452428	31232.076412	30.790093
475.125380	31285.615223	30.795111
476.280851	31349.692739	30.800128
476.490917	31415.321122	30.805146
476.851995	31477.694170	30.810164
477.309424	31531.173557	30.815181
477.736548	31593.621291	30.820199
478.580550	31646.548161	30.825216
478.873720	31711.520315	30.830234
479.455380	31767.623759	30.835252
479.867927	31822.890852	30.840269
480.211272	31891.669756	30.845287
481.049049	31939.973323	30.850304
481.744341	32001.005785	30.855322
481.746764	32057.155353	30.860340
482.612028	32105.896540	30.865357
482.658316	32162.452507	30.870375
483.410504	32212.477839	30.875392
483.956871	32258.571403	30.880410
484.280715	32308.279689	30.885428
484.880955	32373.216188	30.890445
485.200800	32423.547010	30.895463
485.983306	32485.245093	30.900480
485.948279	32535.909347	30.905498
486.162009	32593.928252	30.910516
486.896903	32665.702815	30.915533
487.038353	32724.295701	30.920551
488.146718	32780.851753	30.925568
488.605362	32844.860524	30.930586
489.150642	32896.149336	30.935604
489.691821	32957.494538	30.940621
489.712237	33010.220796	30.945639
490.533754	33077.798944	30.950656
490.599172	33142.971760	30.955674
491.589016	33205.723512	30.960692
492.092953	33274.074261	30.965709
492.122514	33341.424535	30.970727
492.877126	33389.606989	30.975744
493.155161	33466.836837	30.980762
493.886278	33522.148143	30.985780
494.398353	33585.699567	30.990797
494.889092	33656.783305	30.995815
495.472494	33702.820888	31.000832
496.050085	33781.021793	31.005850
496.369574	33844.889938	31.010868
496.876286	33903.300183	31.015885
496.938612	33984.524729	31.020903
497.314614	34042.281774	31.025920
497.813961	34117.136611	31.030938
498.208356	34200.784275	31.035956
498.829748	34270.394252	31.040973
499.494394	34349.665593	31.045991
500.065723	34409.221718	31.051008
500.781999	34487.229280	31.056026
501.292923	34557.839976	31.061044
501.633452	34620.404227	31.066061
502.238127	34693.925107	31.071079
502.986390	34754.361946	31.076096
503.647756	34829.511728	31.081114
504.292296	34879.120620	31.086132
504.959036	34943.096287	31.091149
505.383640	35006.282271	31.096167
505.963385	35058.240625	31.101184
506.072709	35126.023111	31.106202
506.449550	35196.144129	31.111220
507.244350	35258.739723	31.116237
507.830418	35333.607444	31.121255
508.517438	35386.079178	31.126272
508.757310	35462.781235	31.131290
509.060665	35514.016598	31.136308
509.584778	35572.047618	31.141325
509.977190	35645.790513	31.146343
510.725224	35704.551803	31.151360
510.874900	35770.241014	31.156378
511.322193	35856.835123	31.161396
512.267572	35910.679477	31.166413
512.257353	35983.275321	31.171431
513.205238	36055.893082	31.176448
513.597698	36130.057679	31.181466
513.675131	36189.209033	31.186484
514.689872	36269.024364	31.191501
515.120357	36325.422826	31.196519
515.636282	36396.052592	31.201536
516.243766	36451.002108	31.206554
516.799453	36514.834491	31.211572
517.055567	36577.990744	31.216589
517.190878	36648.176282	31.221607
518.105852	36708.301863	31.226624
518.606782	36780.065411	31.231642
518.889709	36845.323133	31.236660
519.873645	36892.341081	31.241677
520.011915	36983.009105	31.246695
520.270517	37046.725187	31.251712
521.234030	37106.459065	31.256730
521.468152	37185.507975	31.261748
521.980801	37246.733802	31.266765
522.426412	37332.249664	31.271783
522.928821	37405.634469	31.276800
523.562295	37477.255824	31.281818
524.012778	37543.075412	31.286836
524.828426	37604.463860	31.291853
525.272813	37685.446423	31.296871
526.113321	37750.782598	31.301888
526.894132	37826.086182	31.306906
527.337635	37888.256643	31.311924
528.379107	37953.150072	31.316941
528.529987	38014.005879	31.321959
529.232408	38074.007019	31.326976
529.467022	38139.211128	31.331994
530.048656	38211.008076	31.337012
530.750236	38265.253248	31.342029
531.072909	38349.856870	31.347047
531.486453	38404.790731	31.352064
532.143804	38465.570715	31.357082
532.413680	38542.164171	31.362100
532.854514	38626.004711	31.367117
533.101054	38695.072019	31.372135
533.613083	38775.379178	31.377152
534.472073	38850.225935	31.382170
534.668015	38932.751167	31.387188
535.563219	38996.744570	31.392205
535.866101	39076.147044	31.397223
536.354278	39165.404713	31.402240
536.659464	39240.038392	31.407258
537.403912	39322.032915	31.412276
538.125989	39396.320622	31.417293
538.558510	39492.144757	31.422311
539.089544	39557.768986	31.427328
539.849348	39637.799152	31.432346
540.016030	39719.701516	31.437364
540.739461	39785.237973	31.442381
541.072088	39862.315867	31.447399
541.895563	39960.312621	31.452416
542.319736	40038.395661	31.457434
542.614215	40115.029556	31.462452
543.733704	40199.339729	31.467469
544.221488	40282.832943	31.472487
544.572982	40356.462945	31.477504
545.404669	40423.322163	31.482522
545.818025	40506.929702	31.487540
546.708460	40572.005805	31.492557
547.350449	40656.482186	31.497575
547.627160	40724.204365	31.502592
547.974845	40796.738292	31.507610
548.563200	40884.548440	31.512628
549.242955	40946.863952	31.517645
549.539866	41031.519011	31.522663
550.002019	41108.104119	31.527680
551.047616	41185.385494	31.532698
551.217483	41262.486705	31.537716
551.844621	41332.205066	31.542733
552.426089	41407.587975	31.547751
553.087855	41476.221587	31.552768
553.430473	41548.929786	31.557786
553.684383	41622.890352	31.562804
554.415380	41691.784810	31.567821
554.793095	41780.779926	31.572839
555.215675	41850.451967	31.577856
556.092159	41916.583190	31.582874
556.432118	42005.175250	31.587892
557.109360	42089.598743	31.592909
557.507919	42164.307848	31.597927
557.958787	42243.147188	31.602944
558.532904	42325.063349	31.607962
559.214749	42407.328273	31.612980
559.944109	42491.066279	31.617997
560.330281	42573.993211	31.623015
560.925113	42654.625728	31.628032
561.575772	42736.944627	31.633050
561.974723	42826.443229	31.638068
562.610419	42904.071026	31.643085
563.361531	42987.207876	31.648103
564.063632	43063.622584	31.653120
564.947850	43150.444438	31.658138
565.254483	43224.901519	31.663156
565.661376	43305.103840	31.668173
566.675275	43386.077584	31.673191
566.851465	43460.673965	31.678208
567.359973	43538.173893	31.683226
567.759194	43634.811241	31.688244
568.203048	43711.201820	31.693261
568.836618	43800.413813	31.698279
569.240653	43899.687899	31.703296
570.077002	43981.296573	31.708314
570.462748	44069.231121	31.713332
571.107096	44149.811456	31.718349
571.848909	44251.424737	31.723367
572.600128	44341.352355	31.728384
573.354247	44421.129601	31.733402
573.659196	44501.208695	31.738420
574.082166	44588.940647	31.743437
575.030351	44666.167442	31.748455
575.433658	44760.489408	31.753472
575.929225	44844.516608	31.758490
576.475886	44936.286830	31.763508
576.955095	45010.372100	31.768525
577.732831	45105.780060	31.773543
578.291478	45189.324800	31.778560
579.184127	45268.940717	31.783578
579.397351	45366.523919	31.788596
579.836450	45450.174818	31.793613
580.534579	45528.403160	31.798631
581.190983	45632.560804	31.803648
581.906035	45715.412697	31.808666
582.212611	45812.903872	31.813684
582.668767	45912.180055	31.818701
582.927976	45997.085031	31.823719
583.659930	46085.874921	31.828736
584.530995	46181.115075	31.833754
585.020332	46272.228772	31.838772
585.538842	46373.568408	31.843789
586.494176	46462.642095	31.848807
587.372708	46550.595333	31.853824
587.928987	46621.295681	31.858842
588.525782	46703.767303	31.863860
589.615344	46784.468598	31.868877
590.062963	46863.580639	31.873895
590.220824	46939.744305	31.878912
590.745416	47022.453438	31.883930
591.224989	47110.143635	31.888948
591.919834	47182.544112	31.893965
592.814568	47264.406921	31.898983
593.139228	47335.495546	31.904000
593.857909	47406.052025	31.909018
594.490425	47493.987148	31.914036
595.074214	47568.510473	31.919053
595.787935	47636.829820	31.924071
595.886106	47731.886542	31.929088
596.638802	47797.989621	31.934106
597.050817	47888.337621	31.939124
597.765499	47977.947668	31.944141
598.335115	48050.751089	31.949159
598.464293	48153.740324	31.954176
599.208888	48228.776517	31.959194
599.230692	48323.160412	31.964212
600.194983	48435.455167	31.969229
600.940759	48516.558536	31.974247
601.224861	48620.311022	31.979264
602.001149	48720.509097	31.984282
602.441078	48812.773732	31.989300
603.126549	48904.739311	31.994317
603.681273	49015.507228	31.999335
604.615933	49101.978831	32.004352
605.399672	49196.838074	32.009370
606.253964	49305.034976	32.014388
606.619598	49382.611025	32.019405
607.478096	49475.482396	32.024423
608.076101	49574.811219	32.029440
608.594996	49653.443106	32.034458
609.061928	49751.411269	32.039476
609.631560	49847.632341	32.044493
610.345035	49941.565784	32.049511
610.894875	50045.847437	32.054528
611.596644	50138.634227	32.059546
612.549777	50219.925354	32.064564
613.193242	50316.850334	32.069581
614.135313	50402.909732	32.074599
614.801824	50493.423862	32.079616
615.263018	50583.628085	32.084634
615.898385	50661.619555	32.089652
616.440112	50759.495251	32.094669
616.811244	50840.307176	32.099687
617.271067	50927.955062	32.104704
618.390447	51021.747807	32.109722
618.513888	51110.731185	32.114740
618.703992	51205.663690	32.119757
619.633558	51304.157142	32.124775
619.988788	51414.201256	32.129792
620.964440	51506.763084	32.134810
621.437803	51612.183934	32.139828
621.674596	51702.187269	32.144845
622.326410	51812.140454	32.149863
622.837062	51918.068478	32.154880
623.700248	52021.750060	32.159898
624.437092	52127.613451	32.164916
625.075524	52241.851005	32.169933
625.673382	52329.185568	32.174951
625.679110	52436.099991	32.179968
626.483709	52529.143482	32.184986
627.456309	52635.362373	32.190004
627.626162	52756.035334	32.195021
628.577335	52852.138925	32.200039
629.404155	52959.893470	32.205056
629.963826	53055.797407	32.210074
630.711554	53168.594681	32.215092
630.973397	53269.185726	32.220109
631.914785	53366.057871	32.225127
632.154167	53477.146772	32.230144
633.113312	53567.459573	32.235162
633.887777	53661.227334	32.240180
634.276493	53774.554903	32.245197
635.045982	53851.052492	32.250215
635.401313	53955.080982	32.255232
636.026591	54066.905519	32.260250
636.329022	54161.101108	32.265268
636.929893	54276.285509	32.270285
637.598534	54381.667038	32.275303
638.213415	54491.164508	32.280320
638.656313	54594.474360	32.285338
639.939684	54703.609908	32.290356
640.406974	54815.287921	32.295373
641.028959	54914.040028	32.300391
641.742081	55025.874494	32.305408
642.747198	55129.574474	32.310426
643.217361	55242.998186	32.315444
643.814551	55352.275946	32.320461
644.647275	55452.657585	32.325479
645.297378	55555.755059	32.330496
645.886434	55666.640689	32.335514
646.426548	55761.367021	32.340532
646.654760	55891.185663	32.345549
647.703594	55988.109916	32.350567
648.175872	56102.037367	32.355584
649.154366	56212.672209	32.360602
649.675747	56325.392377	32.365620
649.898928	56435.780433	32.370637
650.787133	56550.798035	32.375655
651.827493	56663.327009	32.380672
652.124146	56774.178699	32.385690
653.121744	56883.771609	32.390708
653.707779	56993.679517	32.395725
654.461818	57100.464213	32.400743
655.247276	57209.936001	32.405760
655.873847	57305.040890	32.410778
656.577983	57426.918058	32.415796
657.204457	57538.673666	32.420813
657.814612	57643.930661	32.425831
658.522619	57751.630039	32.430848
658.974897	57858.923602	32.435866
659.937882	57983.876588	32.440884
660.342501	58092.120780	32.445901
661.300935	58189.550978	32.450919
661.938485	58306.016625	32.455936
662.465383	58407.727549	32.460954
663.383381	58507.188038	32.465972
663.869240	58632.331311	32.470989
664.991253	58730.988305	32.476007
665.293938	58837.869509	32.481024
666.249385	58950.444421	32.486042
667.067711	59043.845064	32.491060
667.406844	59160.213317	32.496077
667.853698	59258.952824	32.501095
668.553718	59372.261086	32.506112
668.965755	59484.840278	32.511130
669.729196	59592.875357	32.516148
670.210107	59712.736938	32.521165
671.219418	59829.112140	32.526183
671.952262	59934.354624	32.531200
672.379784	60059.364777	32.536218
673.447244	60160.691996	32.541236
673.724509	60272.324656	32.546253
674.247187	60388.025118	32.551271
675.135931	60495.564068	32.556288
675.806762	60604.782684	32.561306
676.700413	60712.587407	32.566324
676.969020	60820.691842	32.571341
677.597066	60923.315167	32.576359
678.418871	61036.846522	32.581376
679.192293	61141.526149	32.586394
679.921279	61248.349759	32.591412
680.181759	61354.524522	32.596429
681.183949	61459.047935	32.601447
681.647662	61568.830517	32.606464
682.356351	61679.356911	32.611482
683.266519	61780.617121	32.616500
683.832850	61903.909362	32.621517
684.548227	62012.167574	32.626535
685.137382	62124.593194	32.631552
685.695651	62242.333452	32.636570
686.172143	62354.880073	32.641588
686.749568	62478.041240	32.646605
687.515302	62599.882722	32.651623
688.061578	62732.284455	32.656640
688.767676	62851.109869	32.661658
689.581654	62959.457960	32.666676
689.965737	63097.829990	32.671693
690.356227	63215.925918	32.676711
691.556002	63345.069803	32.681728
692.192612	63478.864603	32.686746
692.885299	63595.294761	32.691764
693.703382	63730.616094	32.696781
694.404408	63853.645049	32.701799
695.377214	63973.362070	32.706816
695.886167	64120.234332	32.711834
696.644210	64233.939414	32.716852
697.186595	64365.404237	32.721869
698.062152	64502.105418	32.726887
698.921284	64618.526533	32.731904
699.377486	64761.404652	32.736922
700.301449	64879.567430	32.741940
700.933506	65006.223933	32.746957
701.953265	65126.793248	32.751975
702.867061	65246.767624	32.756992
703.501727	65376.377904	32.762010
704.208725	65486.425766	32.767028
705.015114	65613.771493	32.772045
705.713315	65737.159826	32.777063
706.549785	65851.941804	32.782080
707.094485	65981.400055	32.787098
708.090708	66085.790037	32.792116
708.341317	66219.343985	32.797133
709.028439	66342.402716	32.802151
709.822916	66461.405052	32.807168
710.216104	66586.555593	32.812186
711.181437	66698.210805	32.817204
711.765727	66832.434235	32.822221
712.282620	66964.646752	32.827239
713.338909	67076.605052	32.832256
714.017211	67212.263053	32.837274
714.538837	67339.400870	32.842292
715.637350	67467.190157	32.847309
716.390407	67584.441980	32.852327
716.952130	67712.839800	32.857344
717.497599	67848.726166	32.862362
718.531572	67963.152105	32.867380
719.048333	68083.107257	32.872397
719.848565	68205.007701	32.877415
720.703653	68332.557983	32.882432
721.142760	68455.151715	32.887450
721.899171	68582.745100	32.892468
722.520002	68717.107344	32.897485
723.230978	68844.501189	32.902503
723.904558	68970.403622	32.907520
724.384948	69102.559784	32.912538
725.058269	69209.958530	32.917556
725.357740	69347.640150	32.922573
726.089026	69463.028327	32.927591
727.001724	69597.234178	32.932608
727.480875	69739.295374	32.937626
728.520785	69860.375514	32.942644
729.495011	69997.671749	32.947661
729.711670	70125.376237	32.952679
731.056183	70259.533946	32.957696
731.588032	70387.782287	32.962714
732.849893	70511.326927	32.967732
733.489414	70632.825344	32.972749
734.069383	70755.314313	32.977767
734.888870	70893.191972	32.982784
735.658690	71014.519306	32.987802
736.907093	71137.835867	32.992820
737.566052	71268.686182	32.997837
738.322752	71386.521251	33.002855
739.291072	71506.427565	33.007872
739.780395	71639.552812	33.012890
740.679532	71750.531223	33.017908
741.361571	71880.888281	33.022925
741.864869	72000.861515	33.027943
742.401767	72118.319591	33.032960
743.451762	72248.472693	33.037978
744.093267	72380.015590	33.042996
744.507146	72525.406849	33.048013
744.859017	72652.427537	33.053031
745.714116	72786.435348	33.058048
746.355672	72933.461125	33.063066
747.028280	73080.071756	33.068084
747.674799	73215.741800	33.073101
748.432032	73369.384747	33.078119
749.197335	73505.840084	33.083136
750.059654	73654.585940	33.088154
750.676037	73789.467796	33.093172
751.496670	73933.606216	33.098189
751.863583	74090.904262	33.103207
752.791958	74229.006691	33.108224
753.264472	74392.322339	33.113242
754.286371	74541.288238	33.118260
755.014896	74685.763061	33.123277
755.936151	74844.138618	33.128295
757.069777	74999.160174	33.133312
757.742374	75142.983253	33.138330
758.495891	75289.038957	33.143348
759.039114	75433.549341	33.148365
759.951310	75582.293842	33.153383
760.771320	75742.039684	33.158400
761.325440	75885.438202	33.163418
761.987169	76031.336948	33.168436
763.075084	76188.543725	33.173453
763.622528	76339.668306	33.178471
764.582187	76485.773854	33.183488
765.466372	76634.384667	33.188506
765.900688	76787.858409	33.193524
767.032845	76940.256657	33.198541
767.438244	77092.200435	33.203559
768.382581	77239.603736	33.208576
769.045803	77394.511216	33.213594
769.976139	77542.310982	33.218612
770.756641	77687.005731	33.223629
771.487048	77845.105598	33.228647
772.378607	78001.200311	33.233664
773.225537	78146.873773	33.238682
774.175758	78280.292428	33.243700
774.847382	78419.785570	33.248717
775.414443	78561.453678	33.253735
776.341756	78697.870349	33.258752
776.723456	78848.103362	33.263770
777.464510	78982.908020	33.268788
778.716843	79116.193258	33.273805
779.102891	79265.618751	33.278823
779.552566	79406.951088	33.283840
780.599658	79568.034384	33.288858
781.020912	79707.880554	33.293876
782.136093	79848.675670	33.298893
782.657479	80019.526828	33.303911
783.749743	80164.451882	33.308928
784.391749	80313.310771	33.313946
784.996480	80476.339672	33.318964
786.429247	80621.470800	33.323981
786.729617	80774.127575	33.328999
787.878197	80920.964878	33.334016
788.450303	81078.633050	33.339034
789.093706	81229.737077	33.344052
789.959318	81383.158617	33.349069
790.780339	81555.907664	33.354087
791.559374	81696.668656	33.359104
792.046829	81857.278800	33.364122
792.763246	82032.661369	33.369140
794.024533	82180.386544	33.374157
794.560544	82352.714286	33.379175
795.353835	82512.139878	33.384192
796.214229	82676.572145	33.389210
797.055639	82841.888078	33.394228
798.296890	82997.105770	33.399245
798.609231	83174.227677	33.404263
799.851690	83316.016637	33.409280
800.725882	83479.301031	33.414298
801.207989	83652.394023	33.419316
802.477340	83802.279383	33.424333
803.170897	83958.201393	33.429351
804.024858	84111.776135	33.434368
804.684464	84280.359042	33.439386
805.070030	84440.814421	33.444404
806.181018	84597.140017	33.449421
806.778933	84772.329125	33.454439
807.551550	84929.763094	33.459456
808.637504	85108.258994	33.464474
809.379319	85272.223343	33.469492
809.910494	85432.977934	33.474509
810.985880	85602.906444	33.479527
811.652491	85773.112494	33.484544
812.500955	85938.620404	33.489562
813.035228	86118.746352	33.494580
814.268237	86281.852189	33.499597
815.076845	86449.262141	33.504615
815.873806	86620.939778	33.509632
816.732876	86794.304139	33.514650
817.415603	86953.038492	33.519668
818.395101	87117.887780	33.524685
819.213079	87292.458504	33.529703
820.581670	87446.438640	33.534720
821.473893	87623.479944	33.539738
822.409687	87779.242165	33.544756
823.207408	87918.329717	33.549773
823.807694	88081.786747	33.554791
824.880518	88245.015026	33.559808
825.985354	88404.803203	33.564826
826.627713	88551.424835	33.569844
827.608638	88713.165536	33.574861
828.499228	88865.734237	33.579879
829.351808	89010.172548	33.584896
829.837188	89164.923607	33.589914
830.439121	89302.602581	33.594932
831.178063	89443.442715	33.599949
832.144795	89619.119893	33.604967
832.955057	89755.482512	33.609984
833.540772	89907.494459	33.615002
834.194758	90074.310334	33.620020
834.835824	90220.626129	33.625037
835.424564	90394.681836	33.630055
836.515429	90548.905304	33.635072
837.078097	90709.007411	33.640090
837.795953	90893.151792	33.645108
838.844251	91050.891463	33.650125
839.865884	91223.312294	33.655143
840.123145	91391.709077	33.660160
841.140328	91555.494619	33.665178
841.989481	91745.003156	33.670196
843.244211	91910.846674	33.675213
843.765521	92096.216224	33.680231
844.409454	92258.859419	33.685248
845.308729	92434.587455	33.690266
845.880213	92635.983705	33.695284
846.576488	92803.033135	33.700301
847.606979	92982.642094	33.705319
848.519008	93181.569014	33.710336
849.315138	93356.162589	33.715354
850.312231	93549.205146	33.720372
851.445892	93722.619054	33.725389
852.800660	93907.301594	33.730407
853.519233	94080.546090	33.735424
854.804159	94250.337466	33.740442
855.719506	94421.539193	33.745460
856.702485	94586.325654	33.750477
857.486890	94767.210020	33.755495
858.360082	94928.788930	33.760512
859.508794	95104.267263	33.765530
859.939361	95275.453752	33.770548
861.085952	95427.787683	33.775565
861.636820	95612.419655	33.780583
862.659093	95787.005961	33.785600
863.639911	95950.890495	33.790618
864.253164	96136.028806	33.795636
865.394914	96302.965371	33.800653
866.148482	96478.290897	33.805671
866.658554	96657.417825	33.810688
867.759635	96833.967133	33.815706
868.350610	97009.911962	33.820724
869.292753	97189.718338	33.825741
870.111411	97375.021916	33.830759
870.965648	97549.483850	33.835776
871.761161	97735.794099	33.840794
872.157832	97921.677842	33.845812
873.096542	98102.396610	33.850829
874.264340	98287.946863	33.855847
875.111981	98496.176023	33.860864
876.114284	98663.322415	33.865882
876.904674	98860.327615	33.870900
877.790977	99042.397560	33.875917
878.468079	99221.667289	33.880935
879.179178	99428.894870	33.885952
880.389425	99607.699489	33.890970
881.295875	99790.391931	33.895988
882.250459	99981.953426	33.901005
883.106132	100178.489703	33.906023
883.904102	100350.840639	33.911040
885.436796	100535.277341	33.916058
885.820666	100724.267071	33.921076
887.178553	100898.460215	33.926093
887.862191	101080.407399	33.931111
888.750145	101244.766168	33.936128
889.813441	101413.389523	33.941146
890.374569	101594.771824	33.946164
891.381030	101766.287563	33.951181
892.269955	101948.055104	33.956199
892.864163	102116.222406	33.961216
893.820119	102288.503411	33.966234
894.469397	102466.907970	33.971252
895.577085	102652.861075	33.976269
896.602602	102839.747153	33.981287
897.486859	103027.835571	33.986304
898.192216	103198.929428	33.991322
898.913374	103382.577311	33.996340
899.864210	103577.756443	34.001357
900.640801	103757.225306	34.006375
901.500032	103957.126854	34.011392
902.524756	104163.486344	34.016410
902.929049	104357.786510	34.021428
903.615340	104540.327641	34.026445
904.608659	104747.539098	34.031463
905.513258	104947.953674	34.036480
906.414123	105155.797846	34.041498
907.096074	105362.989625	34.046516
908.279997	105566.079283	34.051533
909.320912	105772.043598	34.056551
909.893370	105981.303639	34.061568
911.079381	106182.789358	34.066586
912.250239	106404.441172	34.071604
912.972723	106606.247299	34.076621
914.127341	106812.669600	34.081639
914.832225	107025.436900	34.086656
915.497081	107227.155974	34.091674
916.284143	107452.413503	34.096692
917.706931	107659.925343	34.101709
918.879867	107876.751069	34.106727
919.905840	108079.569553	34.111744
920.786124	108287.061880	34.116762
921.597550	108493.819923	34.121780
922.842534	108705.561602	34.126797
923.529095	108910.950265	34.131815
924.290767	109127.588093	34.136832
925.503972	109331.208465	34.141850
925.764452	109541.878043	34.146868
926.657930	109763.046373	34.151885
927.948068	109974.461306	34.156903
928.762399	110192.124999	34.161920
929.877285	110412.742788	34.166938
931.090259	110620.476908	34.171956
931.963057	110827.952121	34.176973
933.232540	111053.489630	34.181991
934.053820	111272.465552	34.187008
935.130262	111472.463930	34.192026
935.638864	111673.330225	34.197044
936.788889	111891.408157	34.202061
937.879775	112090.331976	34.207079
938.315612	112313.066083	34.212096
939.681425	112520.042106	34.217114
940.615935	112739.023774	34.222132
941.496776	112955.583853	34.227149
942.670600	113156.047178	34.232167
943.121589	113361.546443	34.237184
944.670199	113573.440699	34.242202
945.816523	113790.660253	34.247220
946.205422	114009.311391	34.252237
946.718483	114210.790914	34.257255
947.248665	114422.112391	34.262272
948.452917	114649.869203	34.267290
949.527005	114862.991836	34.272308
950.781742	115060.896554	34.277325
951.762790	115275.025857	34.282343
952.632110	115474.897458	34.287360
953.467144	115686.051502	34.292378
954.797069	115901.014826	34.297396
955.732231	116095.419633	34.302413
956.688009	116297.829325	34.307431
957.475774	116518.626044	34.312448
958.636814	116715.316329	34.317466
959.531441	116921.516083	34.322484
960.017638	117138.110489	34.327501
961.341787	117345.712097	34.332519
962.053777	117565.110501	34.337536
963.284384	117778.964260	34.342554
963.554753	117999.427181	34.347572
964.451727	118222.981215	34.352589
965.744326	118446.357653	34.357607
966.511790	118676.094326	34.362624
967.194402	118887.816909	34.367642
968.532015	119128.638352	34.372660
969.368824	119352.337853	34.377677
970.566465	119570.024306	34.382695
971.175947	119818.928930	34.387712
972.514740	120040.206806	34.392730
973.408511	120267.984035	34.397748
974.320087	120499.764179	34.402765
975.623235	120730.885984	34.407783
976.572640	120966.350926	34.412800
977.937754	121188.026035	34.417818
978.990193	121408.461965	34.422836
980.548030	121628.550019	34.427853
981.555967	121849.364102	34.432871
982.529590	122059.832690	34.437888
983.667311	122269.299965	34.442906
984.591970	122493.959554	34.447924
985.213324	122714.387784	34.452941
986.510094	122925.556876	34.457959
987.466477	123160.354018	34.462976
988.435732	123373.012345	34.467994
989.463519	123587.347970	34.473012
990.284374	123819.372113	34.478029
991.457223	124031.000422	34.483047
992.371768	124253.089838	34.488064
993.197277	124479.453669	34.493082
994.100013	124700.116340	34.498100
994.817811	124940.517664	34.503117
996.081503	125155.636701	34.508135
996.887778	125382.530138	34.513152
998.019096	125625.149853	34.518170
999.253475	125849.175341	34.523188
999.896323	126077.672499	34.528205
1000.879102	126308.092342	34.533223
1001.731473	126541.665864	34.538240
1002.827857	126780.942116	34.543258
1003.770513	127011.196498	34.548276
1004.475209	127248.741411	34.553293
1006.000865	127481.818116	34.558311
1007.025579	127719.149100	34.563328
1007.888234	127957.826804	34.568346
1009.005501	128192.180404	34.573364
1009.976107	128426.940240	34.578381
1011.195313	128656.540314	34.583399
1011.726198	128897.472790	34.588416
1012.872092	129135.529846	34.593434
1013.747413	129378.348445	34.598452
1014.791745	129608.275990	34.603469
1016.153201	129831.802700	34.608487
1017.176258	130058.758466	34.613504
1018.330526	130292.462786	34.618522
1019.241304	130504.648373	34.623540
1020.165328	130720.851311	34.628557
1021.012067	130948.780639	34.633575
1021.764894	131174.622984	34.638592
1022.844114	131392.313327	34.643610
1024.011137	131633.009835	34.648628
1024.689804	131866.981876	34.653645
1025.906736	132107.128704	34.658663
1026.596623	132339.124942	34.663680
1027.346082	132584.486360	34.668698
1028.717592	132826.032846	34.673716
1029.286092	133076.067433	34.678733
1030.583557	133303.495666	34.683751
1031.207409	133568.483150	34.688768
1031.965400	133813.320206	34.693786
1033.332971	134069.252040	34.698804
1033.950054	134338.658506	34.703821
1035.811663	134579.959854	34.708839
1036.852697	134842.353592	34.713856
1038.060303	135093.984436	34.718874
1039.106254	135352.083952	34.723892
1039.930373	135613.670375	34.728909
1041.504466	135855.814698	34.733927
1042.434978	136118.046837	34.738944
1043.476147	136367.471095	34.743962
1044.817569	136617.760482	34.748980
1045.625839	136874.275859	34.753997
1046.447371	137128.445634	34.759015
1047.813459	137385.798401	34.764032
1048.477562	137642.432308	34.769050
1049.543679	137908.954234	34.774068
1050.587831	138173.770359	34.779085
1051.560884	138436.749285	34.784103
1052.109316	138696.161654	34.789120
1053.237058	138959.588276	34.794138
1054.530296	139248.030117	34.799156
1055.565527	139517.511475	34.804173
1056.665641	139788.163425	34.809191
1057.693682	140059.653587	34.814208
1058.805006	140329.483899	34.819226
1059.805587	140587.695116	34.824244
1061.100672	140872.790573	34.829261
1061.905953	141149.968559	34.834279
1062.974795	141426.014851	34.839296
1063.964549	141706.298753	34.844314
1065.504512	141976.882877	34.849332
1066.459909	142257.709515	34.854349
1067.100298	142528.991730	34.859367
1068.190816	142820.832211	34.864384
1069.448219	143096.429691	34.869402
1070.414786	143385.746693	34.874420
1071.093647	143662.839013	34.879437
1072.636084	143941.680368	34.884455
1073.797446	144221.791516	34.889472
1074.808259	144508.270097	34.894490
1075.970535	144774.259258	34.899508
1076.797943	145070.004300	34.904525
1078.085809	145349.025695	34.909543
1079.228162	145633.843206	34.914560
1080.166758	145916.274543	34.919578
1081.565168	146200.559776	34.924596
1082.738199	146493.862904	34.929613
1083.545593	146764.998172	34.934631
1084.639803	147049.124807	34.939648
1085.581307	147342.625302	34.944666
1086.976094	147619.719234	34.949684
1087.560027	147896.010696	34.954701
1088.759135	148154.701603	34.959719
1089.637552	148436.883747	34.964736
1091.057351	148720.386436	34.969754
1091.974000	148987.221131	34.974772
1092.965762	149275.237591	34.979789
1094.083289	149543.425570	34.984807
1095.444947	149806.527560	34.989824
1096.328354	150091.816217	34.994842
1097.451181	150370.967167	34.999860
1098.292470	150658.905174	35.004877
1099.222543	150942.176129	35.009895
1100.850743	151223.888138	35.014912
1101.870213	151514.834617	35.019930
1103.185258	151791.744981	35.024948
1104.032659	152082.686240	35.029965
1105.137890	152365.469809	35.034983
1106.506016	152649.214105	35.040000
1107.316621	152950.809621	35.045018
1108.797352	153223.378072	35.050036
1109.687138	153524.762151	35.055053
1111.055353	153810.366975	35.060071
1112.037337	154092.219818	35.065088
1113.314315	154388.409797	35.070106
1114.992163	154681.720004	35.075124
1115.709438	154966.920866	35.080141
1116.786752	155250.631072	35.085159
1118.312809	155534.104389	35.090176
1119.051418	155835.036878	35.095194
1120.152860	156123.912116	35.100212
1121.052456	156423.401900	35.105229
1122.065665	156724.397407	35.110247
1123.253677	157016.347373	35.115264
1124.156795	157322.503046	35.120282
1125.340109	157623.769119	35.125300
1126.442371	157931.241266	35.130317
1127.459639	158228.480074	35.135335
1128.869639	158542.286879	35.140352
1129.835363	158853.480158	35.145370
1131.511479	159152.532614	35.150388
1132.108674	159457.740375	35.155405
1134.030099	159749.640092	35.160423
1135.883863	160036.466042	35.165440
1136.716614	160347.768944	35.170458
1138.197947	160615.568039	35.175476
1139.191024	160916.344750	35.180493
1140.293487	161203.848464	35.185511
1141.350114	161487.961819	35.190528
1142.598731	161780.317011	35.195546
1143.646292	162059.881378	35.200564
1145.254516	162364.296992	35.205581
1146.200722	162664.764372	35.210599
1147.347369	162946.779591	35.215616
1148.046848	163235.455029	35.220634
1149.310129	163527.135016	35.225652
1150.181240	163824.793942	35.230669
1151.322545	164122.346938	35.235687
1152.634768	164418.960337	35.240704
1153.125990	164726.330640	35.245722
1154.438255	165035.521503	35.250740
1155.662757	165332.308011	35.255757
1156.301750	165642.895850	35.260775
1157.444121	165946.868679	35.265792
1158.516946	166264.570643	35.270810
1159.902421	166584.621348	35.275828
1160.671229	166899.307689	35.280845
1161.885391	167211.448621	35.285863
1163.041505	167534.437063	35.290880
1163.738814	167844.295144	35.295898
1164.927898	168150.534188	35.300916
1166.579253	168462.446917	35.305933
1167.002346	168770.390068	35.310951
1168.820277	169079.640438	35.315968
1169.543014	169398.019273	35.320986
1170.993071	169711.496646	35.326004
1172.015642	170032.406328	35.331021
1173.096255	170345.644581	35.336039
1174.681925	170670.945071	35.341056
1175.377865	170992.943313	35.346074
1176.309866	171303.789095	35.351092
1177.760495	171634.346740	35.356109
1178.544525	171961.895206	35.361127
1179.563868	172290.599978	35.366144
1180.967735	172637.110584	35.371162
1182.141683	172969.132030	35.376180
1183.504071	173312.126790	35.381197
1184.245561	173668.030653	35.386215
1185.944252	173998.729201	35.391232
1187.059585	174336.150580	35.396250
1188.336626	174674.918215	35.401268
1189.619963	175011.758315	35.406285
1190.733161	175363.831909	35.411303
1192.220286	175704.336153	35.416320
1193.121001	176036.982651	35.421338
1194.667756	176394.004997	35.426356
1195.746885	176726.614107	35.431373
1196.777761	177069.957176	35.436391
1198.333362	177424.447480	35.441408
1199.795533	177769.221796	35.446426
1200.876283	178106.713364	35.451444
1202.539544	178446.649318	35.456461
1203.445657	178794.454230	35.461479
1204.755637	179110.999649	35.466496
1206.012270	179472.914942	35.471514
1207.208275	179810.513256	35.476532
1208.154554	180149.665347	35.481549
1209.493120	180512.006087	35.486567
1210.748884	180837.823521	35.491584
1211.900719	181194.679025	35.496602
1213.160059	181539.703087	35.501620
1214.457153	181888.213529	35.506637
1215.843892	182240.988756	35.511655
1217.231013	182584.729484	35.516672
1218.428541	182931.308758	35.521690
1219.697016	183263.993189	35.526708
1220.975724	183604.496563	35.531725
1222.159147	183951.846424	35.536743
1223.729987	184284.500056	35.541760
1224.727470	184636.632099	35.546778
1225.992453	184972.209033	35.551796
1227.290290	185315.969509	35.556813
1228.246361	185671.097962	35.561831
1229.713709	186011.902807	35.566848
1230.621832	186362.715369	35.571866
1231.628017	186718.223147	35.576884
1232.774470	187056.637665	35.581901
1234.048590	187414.415864	35.586919
1235.583949	187766.200042	35.591936
1236.471770	188120.835102	35.596954
1237.605014	188471.090694	35.601972
1239.449291	188827.197106	35.606989
1239.991297	189176.691480	35.612007
1241.523159	189537.575963	35.617024
1242.544586	189892.390440	35.622042
1243.684339	190250.107178	35.627060
1245.241181	190611.870148	35.632077
1246.460089	190960.171923	35.637095
1248.008452	191294.280084	35.642112
1248.862150	191638.901386	35.647130
1250.095621	191970.374172	35.652148
1251.307666	192315.359177	35.657165
1252.211886	192665.538241	35.662183
1253.429158	193016.378573	35.667200
1254.794403	193369.430775	35.672218
1255.870738	193717.137477	35.677236
1257.085420	194091.609276	35.682253
1258.431510	194450.954814	35.687271
1260.014066	194807.178555	35.692288
1261.003927	195177.212756	35.697306
1262.444003	195534.771770	35.702324
1263.740552	195894.501993	35.707341
1264.613984	196257.947629	35.712359
1266.133674	196619.701776	35.717376
1267.348270	196992.121646	35.722394
1268.608007	197367.710087	35.727412
1270.150688	197729.707920	35.732429
1270.948939	198099.613025	35.737447
1272.576986	198476.975265	35.742464
1273.731908	198846.165550	35.747482
1274.786199	199227.879858	35.752500
1276.491420	199602.582377	35.757517
1277.738314	199973.287251	35.762535
1278.790355	200356.252576	35.767552
1280.015897	200734.620847	35.772570
1281.437172	201108.642227	35.777588
1282.795741	201491.309422	35.782605
1283.706233	201872.097466	35.787623
1285.578865	202265.348976	35.792640
1286.430103	202651.407350	35.797658
1288.028824	203035.503483	35.802676
1289.425959	203416.003754	35.807693
1290.543911	203805.706403	35.812711
1291.761601	204183.320148	35.817728
1293.645497	204569.726343	35.822746
1294.932046	204951.636928	35.827764
1296.625202	205322.537674	35.832781
1297.507628	205707.896260	35.837799
1299.615331	206080.078263	35.842816
1300.948501	206448.047548	35.847834
1302.288973	206842.503681	35.852852
1303.730788	207213.429897	35.857869
1304.741970	207580.962631	35.862887
1305.679389	207965.790371	35.867904
1307.140526	208342.356461	35.872922
1308.233290	208720.166030	35.877940
1309.785672	209098.320578	35.882957
1310.884169	209475.802686	35.887975
1312.584195	209855.536367	35.892992
1314.026897	210233.815984	35.898010
1315.301936	210611.883783	35.903028
1316.893208	210979.006416	35.908045
1317.688329	211362.820116	35.913063
1319.039799	211730.887222	35.918080
1320.573129	212127.928149	35.923098
1321.306982	212502.601950	35.928116
1323.084287	212868.343505	35.933133
1324.377011	213261.772400	35.938151
1325.508990	213652.893150	35.943168
1326.828033	214029.965893	35.948186
1328.169963	214422.604635	35.953204
1329.399206	214799.746294	35.958221
1330.479930	215204.418884	35.963239
1331.617001	215590.925146	35.968256
1332.991329	215963.908041	35.973274
1334.080656	216354.387374	35.978292
1335.772572	216720.641468	35.983309
1337.102660	217108.163559	35.988327
1338.078230	217496.050530	35.993344
1339.400332	217859.677973	35.998362
1340.721512	218279.131136	36.003380
1341.995904	218712.715043	36.008397
1343.139602	219090.345386	36.013415
1344.206350	219491.889431	36.018432
1345.484325	219892.028743	36.023450
1346.945977	220298.615893	36.028468
1348.284164	220686.912849	36.033485
1349.433895	221084.487414	36.038503
1350.748974	221480.690101	36.043520
1352.138128	221903.347446	36.048538
1353.449248	222310.780124	36.053556
1354.775888	222723.393162	36.058573
1356.018987	223142.193509	36.063591
1357.490948	223561.897463	36.068608
1358.846888	223975.145387	36.073626
1360.185093	224388.702564	36.078644
1362.254587	224815.983200	36.083661
1363.342063	225237.052252	36.088679
1364.816159	225645.562486	36.093696
1366.393608	226057.943231	36.098714
1367.608970	226494.489466	36.103732
1369.071688	226903.742523	36.108749
1370.862213	227327.801781	36.113767
1372.295248	227744.276123	36.118784
1373.671960	228164.520362	36.123802
1374.319502	228589.661562	36.128820
1376.100951	229015.836262	36.133837
1377.602295	229434.006709	36.138855
1379.014033	229860.981804	36.143872
1380.774090	230280.585466	36.148890
1381.745357	230705.273713	36.153908
1383.390058	231120.453926	36.158925
1384.900462	231543.607960	36.163943
1385.828048	231974.454277	36.168960
1387.266089	232396.632179	36.173978
1388.406911	232835.345549	36.178996
1390.085502	233260.508966	36.184013
1391.299853	233691.338440	36.189031
1392.559358	234129.197798	36.194048
1394.268410	234565.917364	36.199066
1395.737804	235008.037367	36.204084
1397.395317	235428.993646	36.209101
1398.486936	235874.251939	36.214119
1400.015295	236296.019212	36.219136
1401.881573	236730.229332	36.224154
1402.874296	237172.255998	36.229172
1404.431474	237600.905573	36.234189
1405.770009	238045.468340	36.239207
1406.572098	238471.755244	36.244224
1408.250634	238909.024503	36.249242
1409.494025	239363.817694	36.254260
1411.232010	239793.204594	36.259277
1412.938983	240243.986048	36.264295
1413.568797	240676.174148	36.269312
1415.544556	241119.190971	36.274330
1416.861133	241570.370004	36.279348
1418.644836	242012.632928	36.284365
1419.904317	242447.591191	36.289383
1421.287498	242893.021046	36.294400
1422.536827	243333.825219	36.299418
1423.774946	243786.444193	36.304436
1425.511332	244218.100960	36.309453
1427.075218	244666.374784	36.314471
1428.122600	245092.278771	36.319488
1429.603843	245504.648479	36.324506
1431.003545	245949.090398	36.329524
1432.307716	246373.887124	36.334541
1433.462052	246806.711062	36.339559
1434.929244	247248.832219	36.344576
1436.601115	247669.073849	36.349594
1438.138900	248108.974546	36.354612
1439.142331	248542.486291	36.359629
1440.483940	248985.011617	36.364647
1441.844194	249433.326291	36.369664
1443.506878	249877.882781	36.374682
1444.625259	250332.004925	36.379700
1446.078963	250767.858302	36.384717
1447.723379	251226.695815	36.389735
1448.706606	251688.589678	36.394752
1450.342013	252162.417450	36.399770
1451.513419	252620.242092	36.404788
1453.026764	253078.493380	36.409805
1454.460894	253557.512506	36.414823
1455.968699	254035.198909	36.419840
1457.760943	254502.016986	36.424858
1459.230343	254984.384625	36.429876
1460.680703	255454.536779	36.434893
1462.133581	255930.175900	36.439911
1463.268740	256403.733839	36.444928
1464.831002	256878.999763	36.449946
1466.352861	257362.325403	36.454964
1467.962829	257845.941532	36.459981
1469.386569	258323.034504	36.464999
1470.741228	258807.963223	36.470016
1472.489748	259286.704861	36.475034
1473.893836	259785.140170	36.480052
1475.165464	260274.375989	36.485069
1476.707796	260757.292545	36.490087
1478.253220	261257.457433	36.495104
1479.817072	261748.296231	36.500122
1481.388090	262255.264881	36.505140
1482.815760	262745.414700	36.510157
1484.535866	263239.301233	36.515175
1485.888131	263738.125741	36.520192
1487.744893	264228.890189	36.525210
1488.986680	264723.337765	36.530228
1490.317590	265223.638542	36.535245
1492.305975	265713.796275	36.540263
1493.774267	266202.185098	36.545280
1495.899489	266697.527287	36.550298
1497.411235	267182.605849	36.555316
1498.682954	267665.615181	36.560333
1500.273948	268159.342361	36.565351
1501.628197	268645.106179	36.570368
1503.377644	269131.464807	36.575386
1504.646177	269617.445045	36.580404
1506.139817	270120.839505	36.585421
1507.553835	270600.469309	36.590439
1508.851554	271101.989703	36.595456
1510.583611	271593.378223	36.600474
1512.179751	272091.977547	36.605492
1513.436778	272596.347778	36.610509
1515.587151	273088.884558	36.615527
1516.549454	273580.448112	36.620544
1518.235833	274070.621289	36.625562
1520.210062	274565.826724	36.630580
1521.590289	275055.286726	36.635597
1522.720947	275544.609247	36.640615
1524.316195	276040.509712	36.645632
1526.085577	276533.078192	36.650650
1527.845969	277005.579255	36.655668
1529.349424	277478.071018	36.660685
1531.053874	277949.766626	36.665703
1532.485790	278414.444415	36.670720
1534.145313	278881.192100	36.675738
1535.729174	279358.035983	36.680756
1537.326066	279807.315322	36.685773
1538.421404	280282.942262	36.690791
1539.940627	280757.863123	36.695808
1541.247524	281225.273517	36.700826
1542.549043	281698.932577	36.705844
1543.978476	282184.711471	36.710861
1545.692822	282675.547875	36.715879
1546.652999	283174.381959	36.720896
1548.143939	283669.012027	36.725914
1549.828188	284162.135531	36.730932
1551.403934	284662.972201	36.735949
1552.852872	285163.066278	36.740967
1553.805224	285687.905521	36.745984
1555.205822	286201.263942	36.751002
1556.469208	286730.341299	36.756020
1558.142919	287255.107182	36.761037
1559.715491	287789.235539	36.766055
1561.064471	288324.567338	36.771072
1562.578723	288853.875331	36.776090
1564.193833	289405.161797	36.781108
1565.494290	289950.046279	36.786125
1567.735105	290486.975510	36.791143
1568.614732	291039.164293	36.796160
1570.659621	291580.185600	36.801178
1572.698891	292132.153121	36.806196
1574.323926	292680.503626	36.811213
1575.796000	293228.775413	36.816231
1577.311033	293774.523128	36.821248
1578.729216	294333.898697	36.826266
1580.511916	294885.591644	36.831284
1581.795782	295445.212809	36.836301
1583.444861	296009.215952	36.841319
1584.866520	296578.740117	36.846336
1586.508612	297145.075564	36.851354
1588.247135	297718.580168	36.856372
1589.379767	298291.089605	36.861389
1591.053709	298864.141682	36.866407
1592.660570	299437.862121	36.871424
1594.642280	300009.333320	36.876442
1596.673966	300581.783664	36.881460
1597.962016	301146.251470	36.886477
1599.652702	301714.434001	36.891495
1601.260759	302302.665887	36.896512
1602.927634	302873.055307	36.901530
1604.207848	303430.146009	36.906548
1605.716288	304029.660386	36.911565
1607.187454	304608.757662	36.916583
1608.842315	305190.182959	36.921600
1610.720475	305777.993168	36.926618
1612.657091	306355.351824	36.931636
1613.700859	306957.285645	36.936653
1615.495635	307536.869533	36.941671
1617.341941	308118.447373	36.946688
1618.894516	308708.069532	36.951706
1620.555345	309298.380829	36.956724
1622.146013	309890.197905	36.961741
1623.724050	310470.305472	36.966759
1625.178299	311055.610027	36.971776
1627.132439	311652.687455	36.976794
1628.669420	312237.766613	36.981812
1630.338301	312835.821855	36.986829
1632.237365	313424.184580	36.991847
1633.806055	313996.370274	36.996864
1635.430248	314572.148524	37.001882
1637.318757	315131.169479	37.006900
1638.523246	315692.178269	37.011917
1640.415083	316264.318830	37.016935
1642.007917	316826.194500	37.021952
1643.579649	317378.470638	37.026970
1645.310987	317950.141944	37.031988
1646.645495	318520.731456	37.037005
1648.427750	319082.151896	37.042023
1649.942659	319664.052897	37.047040
1651.472417	320240.791924	37.052058
1653.228433	320812.435749	37.057076
1654.825655	321410.914752	37.062093
1656.515960	321984.590847	37.067111
1658.262998	322561.985177	37.072128
1659.638785	323150.531649	37.077146
1661.496921	323729.243118	37.082164
1662.950069	324340.694085	37.087181
1664.828212	324931.020403	37.092199
1666.125353	325541.114524	37.097216
1667.883039	326134.039289	37.102234
1669.403723	326727.352973	37.107252
1671.274793	327343.656821	37.112269
1672.877926	327948.395787	37.117287
1674.849525	328554.489721	37.122304
1676.143573	329177.141223	37.127322
1677.802617	329792.261797	37.132340
1679.678997	330408.533353	37.137357
1681.239096	331023.428876	37.142375
1683.215317	331640.737222	37.147392
1684.692181	332265.534440	37.152410
1686.280093	332897.034073	37.157428
1688.007821	333516.038656	37.162445
1689.740584	334148.211181	37.167463
1691.566175	334777.543324	37.172480
1693.062797	335416.137647	37.177498
1695.028284	336047.336083	37.182516
1696.578236	336681.540415	37.187533
1698.273119	337315.383339	37.192551
1700.290982	337943.860021	37.197568
1702.042565	338590.954566	37.202586
1703.828427	339215.900498	37.207604
1705.608083	339851.983436	37.212621
1707.452547	340485.407945	37.217639
1709.110285	341115.860194	37.222656
1710.759517	341757.499858	37.227674
1712.230402	342392.205944	37.232692
1714.250670	343040.037468	37.237709
1715.938345	343675.706696	37.242727
1717.778691	344317.180276	37.247744
1719.116639	344952.712949	37.252762
1721.054884	345586.590012	37.257780
1722.873059	346236.899739	37.262797
1724.680527	346870.172239	37.267815
1726.635164	347513.411656	37.272832
1728.372372	348155.815228	37.277850
1730.270316	348783.158961	37.282868
1731.737453	349435.487268	37.287885
1733.407658	350071.226057	37.292903
1735.081141	350715.177955	37.297920
1736.684932	351368.598092	37.302938
1738.607605	351995.360636	37.307956
1740.140175	352659.914361	37.312973
1742.267748	353309.235498	37.317991
1744.091050	353938.346990	37.323008
1745.438536	354598.080501	37.328026
1747.103121	355243.998154	37.333044
1748.653820	355878.632984	37.338061
1750.099334	356520.126946	37.343079
1752.103495	357143.706266	37.348096
1753.773112	357773.269088	37.353114
1755.454962	358412.843029	37.358132
1757.295795	359041.825674	37.363149
1759.323197	359662.141227	37.368167
1761.108890	360308.620936	37.373184
1763.025793	360940.911180	37.378202
1764.822548	361566.437176	37.383220
1765.900083	362210.872235	37.388237
1767.261150	362850.302863	37.393255
1768.920050	363499.771545	37.398272
1770.410295	364173.206698	37.403290
1772.451612	364827.613724	37.408308
1774.295692	365503.124102	37.413325
1775.871403	366159.006265	37.418343
1778.019332	366820.922020	37.423360
1779.448247	367510.748110	37.428378
1781.829924	368181.176091	37.433396
1783.488739	368850.925078	37.438413
1784.996456	369530.275605	37.443431
1786.887579	370212.239351	37.448448
1788.412733	370893.997305	37.453466
1790.600469	371567.643388	37.458484
1792.556591	372281.213823	37.463501
1794.051558	372960.782402	37.468519
1795.726862	373647.638590	37.473536
1797.013406	374358.412526	37.478554
1798.905380	375057.608588	37.483572
1800.963968	375754.734464	37.488589
1802.344433	376474.403497	37.493607
1804.166315	377190.054020	37.498624
1805.657849	377917.131276	37.503642
1807.806645	378627.372628	37.508660
1809.476673	379353.908428	37.513677
1811.594532	380079.416688	37.518695
1813.334109	380816.636783	37.523712
1814.813286	381544.146372	37.528730
1816.770658	382273.615309	37.533748
1818.756943	383018.505849	37.538765
1820.479530	383757.870203	37.543783
1822.396664	384494.548950	37.548800
1823.948660	385243.670037	37.553818
1826.119811	385974.188407	37.558836
1828.070484	386726.150756	37.563853
1829.872529	387464.556089	37.568871
1831.918464	388210.459312	37.573888
1833.351201	388969.730753	37.578906
1835.654440	389699.762240	37.583924
1837.578015	390447.509046	37.588941
1839.117210	391198.267408	37.593959
1841.279595	391938.967805	37.598976
1843.345668	392692.138139	37.603994
1845.218241	393434.472830	37.609012
1847.345350	394174.998544	37.614029
1849.157422	394918.954753	37.619047
1851.186634	395654.821994	37.624064
1852.560518	396403.452358	37.629082
1854.863115	397139.035380	37.634100
1856.736243	397881.210024	37.639117
1858.229828	398642.918295	37.644135
1860.373003	399368.892187	37.649152
1862.021039	400120.297934	37.654170
1864.268550	400858.179429	37.659188
1866.186231	401596.755428	37.664205
1867.700581	402348.987087	37.669223
1869.562652	403084.011693	37.674240
1871.527323	403818.189579	37.679258
1873.378402	404554.140937	37.684276
1875.285940	405266.499238	37.689293
1876.660449	405981.790551	37.694311
1878.792305	406717.740285	37.699328
1880.501119	407438.969278	37.704346
1882.137506	408159.228674	37.709364
1884.060561	408898.093810	37.714381
1885.753151	409637.889074	37.719399
1887.753996	410384.985489	37.724416
1889.561885	411125.253284	37.729434
1891.259809	411864.353637	37.734452
1893.169398	412608.591694	37.739469
1895.067907	413359.168876	37.744487
1897.026239	414106.092810	37.749504
1898.894116	414864.104825	37.754522
1901.085510	415625.638317	37.759540
1903.082972	416380.672402	37.764557
1904.629044	417142.673375	37.769575
1907.034213	417897.900088	37.774592
1908.986165	418660.599865	37.779610
1910.625875	419421.809008	37.784628
1913.032704	420190.035682	37.789645
1914.575113	420957.470090	37.794663
1916.764506	421727.711943	37.799680
1918.347884	422504.765798	37.804698
1920.266930	423274.574363	37.809716
1922.097273	424050.855784	37.814733
1924.138840	424823.406781	37.819751
1926.303221	425599.027560	37.824768
1928.000881	426392.473967	37.829786
1929.916552	427181.200369	37.834804
1931.886128	427966.702501	37.839821
1933.889873	428761.287070	37.844839
1935.811739	429544.568696	37.849856
1937.537769	430344.260339	37.854874
1939.528761	431143.375264	37.859892
1941.690449	431938.840881	37.864909
1943.408043	432750.400258	37.869927
1945.133755	433546.389848	37.874944
1947.361986	434349.963588	37.879962
1949.392788	435172.270506	37.884980
1951.422638	435980.730515	37.889997
1952.618133	436790.059060	37.895015
1955.000864	437609.538715	37.900032
1956.896045	438428.209084	37.905050
1958.823217	439260.559533	37.910068
1961.046394	440089.946071	37.915085
1962.908804	440914.807255	37.920103
1964.701190	441735.652119	37.925120
1966.589009	442569.354258	37.930138
1968.790987	443403.782940	37.935156
1970.843143	444231.779125	37.940173
1972.731566	445069.080676	37.945191
1975.041072	445899.956738	37.950208
1976.589611	446740.741356	37.955226
1978.498593	447572.479785	37.960244
1980.403409	448395.233047	37.965261
1982.417777	449251.879441	37.970279
1984.248508	450086.821791	37.975296
1986.724504	450943.324368	37.980314
1988.298696	451781.277510	37.985332
1990.465189	452628.405974	37.990349
1992.387727	453474.529118	37.995367
1994.299336	454315.208632	38.000384
1996.289629	455179.457939	38.005402
1998.152531	456028.521697	38.010420
2000.684869	456859.387897	38.015437
2002.352240	457726.112471	38.020455
2003.758471	458555.376663	38.025472
2006.399634	459374.948709	38.030490
2008.099149	460221.135668	38.035508
2010.039621	461036.660938	38.040525
2011.741978	461875.396940	38.045543
2013.735439	462713.089417	38.050560
2016.284669	463542.364934	38.055578
2017.989516	464382.158049	38.060596
2019.906413	465227.996674	38.065613
2022.034980	466075.785905	38.070631
2024.096785	466925.975581	38.075648
2026.359529	467767.402451	38.080666
2028.082579	468611.358331	38.085684
2030.307029	469477.228029	38.090701
2031.842070	470330.286846	38.095719
2033.992633	471184.267500	38.100736
2036.003709	472054.351569	38.105754
2037.586145	472945.940100	38.110772
2039.671050	473816.335735	38.115789
2041.712572	474701.450638	38.120807
2043.299283	475594.934558	38.125824
2045.866654	476485.991517	38.130842
2048.055401	477370.350100	38.135860
2050.459185	478258.823643	38.140877
2051.836138	479167.273938	38.145895
2054.177787	480062.489778	38.150912
2056.331278	480965.268632	38.155930
2058.094291	481872.864986	38.160948
2060.717230	482769.669553	38.165965
2062.558959	483690.645420	38.170983
2064.480628	484607.572161	38.176000
2066.965545	485518.855750	38.181018
2068.749011	486445.506735	38.186036
2071.253539	487360.429392	38.191053
2072.809960	488274.603073	38.196071
2075.099764	489201.077357	38.201088
2077.469994	490135.566168	38.206106
2079.446871	491067.596786	38.211124
2082.148442	491975.937879	38.216141
2084.339963	492898.346370	38.221159
2086.533928	493814.043670	38.226176
2088.627249	494733.241527	38.231194
2090.527463	495661.606181	38.236212
2092.693386	496579.633450	38.241229
2094.471027	497504.991540	38.246247
2096.406901	498445.358817	38.251264
2098.467683	499371.779204	38.256282
2100.110342	500317.085234	38.261300
2102.594763	501250.546332	38.266317
2104.757077	502194.601337	38.271335
2106.586231	503141.885877	38.276352
2108.807086	504081.839243	38.281370
2110.515634	505034.835525	38.286388
2112.995230	505990.170986	38.291405
2115.238273	506943.422182	38.296423
2117.656033	507891.294236	38.301440
2120.043505	508833.468709	38.306458
2121.849577	509793.230071	38.311476
2124.127937	510724.925864	38.316493
2126.328068	511679.972240	38.321511
2128.466057	512634.316505	38.326528
2130.752016	513559.544652	38.331546
2132.706364	514520.258139	38.336564
2135.061724	515457.460980	38.341581
2137.062164	516410.390803	38.346599
2139.175479	517361.833071	38.351616
2141.202358	518315.650485	38.356634
2143.295106	519264.006985	38.361652
2145.462222	520198.638659	38.366669
2147.462647	521121.955521	38.371687
2149.176829	522043.652049	38.376704
2151.273695	522967.799307	38.381722
2153.561984	523913.066452	38.386740
2155.590100	524834.190283	38.391757
2157.970353	525772.224346	38.396775
2159.641437	526717.015585	38.401792
2161.901686	527661.348231	38.406810
2163.506256	528614.088979	38.411828
2165.779520	529571.895638	38.416845
2168.095005	530528.072825	38.421863
2170.184692	531498.725914	38.426880
2172.401727	532458.218373	38.431898
2174.666529	533411.398067	38.436916
2176.935543	534391.748201	38.441933
2179.473527	535359.253485	38.446951
2181.206345	536333.471029	38.451968
2183.524785	537312.408444	38.456986
2185.591800	538303.851896	38.462004
2187.954628	539268.809941	38.467021
2190.501902	540262.152639	38.472039
2192.826830	541238.657958	38.477056
2194.938263	542225.344666	38.482074
2196.869863	543218.029328	38.487092
2199.381411	544204.964946	38.492109
2201.450044	545210.414988	38.497127
2203.679810	546212.849235	38.502144
2206.229741	547216.919096	38.507162
2208.053324	548217.516102	38.512180
2209.919278	549214.312861	38.517197
2212.161376	550227.116370	38.522215
2214.597761	551244.137365	38.527232
2217.002517	552252.038790	38.532250
2219.104096	553256.447247	38.537268
2221.365337	554284.531827	38.542285
2224.159418	555304.860943	38.547303
2225.874672	556330.568271	38.552320
2228.794759	557349.465663	38.557338
2230.920849	558373.542395	38.562356
2233.031378	559378.700266	38.567373
2235.516571	560414.671183	38.572391
2237.493919	561430.146964	38.577408
2240.050133	562452.030441	38.582426
2242.001909	563485.337267	38.587444
2244.140021	564507.280931	38.592461
2246.710666	565528.721996	38.597479
2248.352974	566572.936047	38.602496
2251.391252	567604.884520	38.607514
2253.312065	568651.747853	38.612532
2255.090391	569691.369994	38.617549
2257.652484	570737.305548	38.622567
2259.610498	571783.004392	38.627584
2261.977102	572829.905610	38.632602
2264.366734	573885.851956	38.637620
2266.854946	574923.777008	38.642637
2269.107185	575976.008387	38.647655
2271.007856	577041.407132	38.652672
2273.315301	578075.840637	38.657690
2275.406252	579144.089980	38.662708
2277.802544	580198.953357	38.667725
2280.605536	581250.048385	38.672743
2282.867679	582307.764257	38.677760
2285.141674	583361.676082	38.682778
2287.377287	584417.961233	38.687796
2289.404440	585465.263774	38.692813
2292.129762	586526.802061	38.697831
2294.173092	587581.942649	38.702848
2296.466349	588602.158207	38.707866
2298.759007	589633.065345	38.712884
2301.207897	590659.648068	38.717901
2303.469906	591676.099730	38.722919
2305.648404	592695.134944	38.727936
2308.144431	593718.841424	38.732954
2310.334106	594746.819450	38.737972
2312.426055	595772.519893	38.742989
2314.974508	596806.873281	38.748007
2316.842355	597839.845362	38.753024
2319.474454	598871.799080	38.758042
2321.530126	599923.740643	38.763060
2323.331014	600969.118840	38.768077
2326.332442	602029.327955	38.773095
2328.135592	603089.537397	38.778112
2330.519921	604141.042317	38.783130
2332.848450	605206.727994	38.788148
2335.374598	606269.078368	38.793165
2338.400870	607325.941936	38.798183
2340.920383	608396.253890	38.803200
2343.171152	609447.442737	38.808218
2346.046491	610524.050753	38.813236
2348.233727	611569.948635	38.818253
2350.534907	612632.590292	38.823271
2352.550573	613723.341992	38.828288
2354.920707	614789.019035	38.833306
2357.341771	615864.088474	38.838324
2359.707821	616947.764542	38.843341
2361.812841	618038.628183	38.848359
2364.228863	619122.532626	38.853376
2366.803597	620201.054508	38.858394
2369.133857	621301.356150	38.863412
2371.324856	622396.821285	38.868429
2373.913553	623490.061400	38.873447
2376.301484	624591.320350	38.878464
2378.907431	625693.580483	38.883482
2381.321844	626793.910742	38.888500
2383.691181	627903.977735	38.893517
2386.132642	629009.971347	38.898535
2388.188866	630117.861854	38.903552
2390.739379	631224.656496	38.908570
2393.052747	632350.651014	38.913588
2395.274870	633459.613199	38.918605
2398.305604	634581.007065	38.923623
2400.277774	635698.012528	38.928640
2403.275482	636806.293671	38.933658
2405.725060	637930.918582	38.938676
2408.466240	639044.593943	38.943693
2410.994353	640144.362080	38.948711
2413.176318	641266.423641	38.953728
2415.765644	642378.916387	38.958746
2418.332023	643488.349137	38.963764
2420.174327	644601.921004	38.968781
2422.914622	645711.133614	38.973799
2425.362187	646831.344376	38.978816
2427.642256	647946.971274	38.983834
2430.211754	649079.628241	38.988852
2432.534261	650199.486278	38.993869
2434.957217	651308.685244	38.998887
2437.400965	652449.656167	39.003904
2440.017271	653574.271722	39.008922
2442.682478	654696.509743	39.013940
2445.119428	655814.323701	39.018957
2447.659468	656936.129216	39.023975
2449.900897	658057.507586	39.028992
2452.298864	659176.441057	39.034010
2454.664191	660296.447331	39.039028
2456.926523	661418.134779	39.044045
2459.182811	662512.906988	39.049063
2461.515452	663612.969642	39.054080
2463.805740	664696.238345	39.059098
2466.129799	665806.854651	39.064116
2468.621713	666909.252761	39.069133
2471.122372	668016.150555	39.074151
2473.329322	669126.949107	39.079168
2475.601206	670228.254537	39.084186
2478.251480	671352.799549	39.089204
2480.847491	672467.421620	39.094221
2483.766125	673584.942432	39.099239
2485.619200	674723.789252	39.104256
2488.027997	675849.827136	39.109274
2490.651911	676978.428454	39.114292
2492.791049	678131.280645	39.119309
2495.227308	679277.380399	39.124327
2497.470783	680433.259891	39.129344
2499.985674	681594.117975	39.134362
2502.278293	682775.385846	39.139380
2504.936381	683946.406971	39.144397
2507.285377	685118.769898	39.149415
2508.944653	686317.616822	39.154432
2511.552651	687513.865388	39.159450
2514.248378	688710.388783	39.164468
2516.612640	689925.425349	39.169485
2519.463213	691129.744627	39.174503
2521.766252	692341.239085	39.179520
2524.609493	693568.856894	39.184538
2527.226914	694789.148830	39.189556
2529.081982	696013.864319	39.194573
2531.891527	697242.221999	39.199591
2534.573666	698487.789219	39.204608
2536.868289	699718.516414	39.209626
2539.851373	700959.568792	39.214644
2542.415001	702217.469680	39.219661
2545.206418	703459.190994	39.224679
2547.499348	704713.901886	39.229696
2549.900526	705966.035202	39.234714
2552.505323	707217.210791	39.239732
2555.106332	708475.190897	39.244749
2557.502778	709756.152694	39.249767
2560.060511	711032.687072	39.254784
2562.432981	712307.328381	39.259802
2564.875282	713575.826411	39.264820
2567.576019	714868.200547	39.269837
2570.128049	716152.433319	39.274855
2572.683412	717445.328629	39.279872
2575.289154	718738.215033	39.284890
2578.131715	720022.403423	39.289908
2580.571240	721321.102778	39.294925
2583.071818	722620.974656	39.299943
2586.074536	723916.654020	39.304960
2588.575032	725215.377850	39.309978
2591.162435	726509.038660	39.314996
2593.530884	727820.325782	39.320013
2596.263059	729116.567435	39.325031
2598.945753	730416.663578	39.330048
2601.402371	731722.616901	39.335066
2604.252488	733028.147466	39.340084
2606.661903	734349.344127	39.345101
2609.421721	735650.910649	39.350119
2612.206310	736958.039148	39.355136
2614.325791	738288.215503	39.360154
2617.187170	739589.669875	39.365172
2620.343579	740898.018575	39.370189
2622.804323	742208.832326	39.375207
2625.624176	743528.742934	39.380224
2628.673563	744812.834362	39.385242
2630.945757	746074.061655	39.390260
2633.424358	747355.908961	39.395277
2635.847013	748609.998242	39.400295
2638.404863	749880.819697	39.405312
2640.622165	751152.672702	39.410330
2643.314517	752434.882270	39.415348
2645.378954	753726.737566	39.420365
2647.923508	755007.657979	39.425383
2650.424376	756305.363343	39.430400
2652.492144	757615.920160	39.435418
2655.046239	758928.240082	39.440436
2657.336127	760265.432558	39.445453
2660.537438	761578.665712	39.450471
2663.218833	762912.128465	39.455488
2665.503698	764258.655432	39.460506
2668.108502	765598.150159	39.465524
2670.797634	766953.769026	39.470541
2672.936323	768318.821513	39.475559
2675.395127	769698.664328	39.480576
2677.855125	771074.515471	39.485594
2681.016827	772453.337540	39.490612
2683.485556	773862.086877	39.495629
2685.971983	775265.700710	39.500647
2688.795153	776676.505580	39.505664
2691.063282	778098.424519	39.510682
2693.814033	779516.402979	39.515700
2696.352192	780950.927828	39.520717
2698.720899	782384.019092	39.525735
2701.844137	783836.132569	39.530752
2704.328165	785293.062633	39.535770
2706.892969	786744.583038	39.540788
2709.449272	788215.572602	39.545805
2712.180041	789686.132217	39.550823
2715.031840	791149.407530	39.555840
2717.172954	792628.278170	39.560858
2720.382481	794126.114877	39.565876
2723.219126	795610.566348	39.570893
2725.835225	797109.922740	39.575911
2728.480193	798615.808266	39.580928
2731.184958	800117.736251	39.585946
2734.196355	801608.521646	39.590964
2737.211122	803124.039558	39.595981
2740.005809	804644.153446	39.600999
2742.898187	806136.525120	39.606016
2745.643933	807646.738651	39.611034
2748.537706	809157.034352	39.616052
2751.421357	810667.681446	39.621069
2754.205037	812178.400128	39.626087
2757.675105	813687.300730	39.631104
2760.199551	815192.014468	39.636122
2763.010255	816691.363359	39.641140
2765.736348	818214.266287	39.646157
2768.702463	819715.158418	39.651175
2771.389330	821216.832199	39.656192
2774.136347	822727.524585	39.661210
2776.819422	824237.590183	39.666228
2779.776913	825762.724886	39.671245
2782.539684	827265.304591	39.676263
2785.719618	828763.717798	39.681280
2788.057220	830300.622219	39.686298
2791.125472	831804.593722	39.691316
2793.722575	833318.865262	39.696333
2796.309584	834826.599297	39.701351
2799.233900	836349.360218	39.706368
2802.103978	837876.442770	39.711386
2804.633774	839388.812473	39.716404
2807.794349	840909.721668	39.721421
2810.740830	842407.975776	39.726439
2813.777439	843880.913355	39.731456
2816.011018	845356.752431	39.736474
2819.152325	846823.347267	39.741492
2821.765023	848288.715522	39.746509
2824.191467	849762.615134	39.751527
2827.236665	851245.197764	39.756544
2829.537182	852733.475472	39.761562
2832.541481	854220.407104	39.766580
2834.995618	855716.586652	39.771597
2837.643023	857211.692769	39.776615
2840.535216	858706.977958	39.781632
2843.188067	860234.339832	39.786650
2846.088826	861745.956201	39.791668
2848.909213	863259.538564	39.796685
2852.017660	864792.762989	39.801703
2854.736095	866312.193320	39.806720
2857.592542	867861.835803	39.811738
2859.889021	869403.907524	39.816756
2863.155831	870958.012665	39.821773
2865.732986	872511.537840	39.826791
2868.574492	874062.486046	39.831808
2871.143435	875636.298051	39.836826
2873.892592	877206.954421	39.841844
2876.954321	878790.585055	39.846861
2879.455041	880382.101019	39.851879
2882.670911	881972.005049	39.856896
2885.349126	883589.975937	39.861914
2887.893529	885187.137105	39.866932
2890.579542	886796.102261	39.871949
2893.493224	888431.811255	39.876967
2896.525069	890052.463178	39.881984
2899.816501	891688.924696	39.887002
2902.689643	893316.210467	39.892020
2905.488818	894967.252957	39.897037
2908.169418	896614.366718	39.902055
2911.223904	898253.038607	39.907072
2913.823676	899922.050052	39.912090
2917.172269	901563.088104	39.917108
2919.857214	903239.196292	39.922125
2922.653657	904905.158856	39.927143
2925.389078	906571.020764	39.932160
2928.359305	908261.362408	39.937178
2931.445259	909930.299202	39.942196
2934.609874	911625.548079	39.947213
2937.130573	913318.364309	39.952231
2940.225218	915009.316451	39.957248
2943.187135	916701.498772	39.962266
2946.191268	918392.286443	39.967284
2949.708258	920082.465386	39.972301
2952.640858	921776.533973	39.977319
2956.014083	923466.929920	39.982336
2958.892742	925155.823058	39.987354
2961.668125	926850.723583	39.992372
2964.867128	928545.306414	39.997389
2967.962118	930240.519234	40.002407
2970.998222	931917.097124	40.007424
2974.099234	933618.417290	40.012442
2976.814592	935313.797481	40.017460
2979.760826	937005.915353	40.022477
2982.509932	938695.607974	40.027495
2985.798261	940394.040229	40.032512
2988.667567	942089.886138	40.037530
2991.393822	943783.005271	40.042548
2994.676326	945492.297283	40.047565
2997.543523	947194.311535	40.052583
3000.531685	948881.039621	40.057600
3003.716518	950597.536436	40.062618
3006.742232	952286.193984	40.067636
3009.970026	953939.824015	40.072653
3012.707708	955613.873134	40.077671
3016.116625	957299.193979	40.082688
3018.491811	958996.906009	40.087706
3021.417551	960685.717939	40.092724
3024.414827	962385.360445	40.097741
3027.410461	964077.857733	40.102759
3030.103706	965793.251741	40.107776
3033.048544	967509.264414	40.112794
3035.415561	969239.502485	40.117812
3038.487565	970973.299364	40.122829
3041.340729	972713.047196	40.127847
3044.103283	974451.891881	40.132864
3046.904215	976232.614405	40.137882
3049.849810	978001.257841	40.142900
3052.844272	979768.566746	40.147917
3055.778482	981570.990215	40.152935
3058.645577	983356.106930	40.157952
3061.732640	985169.345979	40.162970
3064.477442	987004.933596	40.167988
3067.264072	988831.945506	40.173005
3070.539836	990660.429814	40.178023
3073.377170	992486.064991	40.183040
3076.312415	994346.085541	40.188058
3079.818614	996197.921401	40.193076
3083.277276	998048.383344	40.198093
3086.140446	999915.815917	40.203111
3089.025179	1001780.978930	40.208128
3092.273588	1003647.698710	40.213146
3094.898269	1005536.990017	40.218164
3098.044308	1007440.592860	40.223181
3101.233948	1009342.092227	40.228199
3103.751687	1011228.719738	40.233216
3106.650893	1013148.265134	40.238234
3109.846461	1015074.078864	40.243252
3113.301539	1016981.282093	40.248269
3116.238073	1018918.598260	40.253287
3119.802073	1020847.983970	40.258304
3123.128108	1022788.058786	40.263322
3125.807139	1024719.351554	40.268340
3128.775732	1026660.753108	40.273357
3132.095345	1028612.628305	40.278375
3135.060043	1030562.817720	40.283392
3138.490255	1032526.535721	40.288410
3141.507006	1034477.278510	40.293428
3144.599874	1036439.190751	40.298445
3147.888082	1038408.479347	40.303463
3150.787184	1040371.158067	40.308480
3153.925503	1042340.523850	40.313498
3157.024433	1044322.490501	40.318516
3160.326297	1046295.145264	40.323533
3163.009124	1048282.504648	40.328551
3166.583594	1050262.267938	40.333568
3169.995953	1052251.352746	40.338586
3173.216298	1054230.233662	40.343604
3176.664202	1056208.463681	40.348621
3179.542388	1058204.430145	40.353639
3182.986230	1060174.799159	40.358656
3186.050174	1062156.719401	40.363674
3189.455255	1064159.752891	40.368692
3192.599821	1066136.768965	40.373709
3195.539660	1068125.383328	40.378727
3198.894919	1070122.603992	40.383744
3201.761379	1072106.046545	40.388762
3204.816307	1074101.194192	40.393780
3208.203915	1076104.274262	40.398797
3210.932266	1078110.366336	40.403815
3214.301121	1080095.900810	40.408832
3217.233036	1082067.199284	40.413850
3220.065259	1084019.917291	40.418868
3223.366528	1085972.430895	40.423885
3226.218583	1087946.201477	40.428903
3229.338870	1089918.732956	40.433920
3232.127821	1091880.192979	40.438938
3235.301517	1093878.968554	40.443956
3238.662014	1095854.264561	40.448973
3241.913224	1097864.628595	40.453991
3245.104968	1099861.286546	40.459008
3248.310905	1101871.787698	40.464026
3251.180222	1103887.312041	40.469044
3254.848694	1105913.666490	40.474061
3257.652561	1107936.734783	40.479079
3260.490713	1109977.405490	40.484096
3263.756852	1112019.989856	40.489114
3266.762503	1114087.137311	40.494132
3269.977533	1116148.795332	40.499149
3272.929306	1118231.370063	40.504167
3276.277974	1120317.723758	40.509184
3280.022014	1122394.557343	40.514202
3282.738961	1124500.556769	40.519220
3286.429964	1126600.725776	40.524237
3289.894681	1128702.949872	40.529255
3292.903362	1130813.330870	40.534272
3296.689513	1132929.948978	40.539290
3299.840237	1135056.248919	40.544308
3302.927719	1137169.303056	40.549325
3306.390636	1139303.791760	40.554343
3309.552210	1141436.618550	40.559360
3313.106677	1143570.980109	40.564378
3316.314712	1145717.205243	40.569396
3319.693213	1147862.246605	40.574413
3323.100062	1150014.723784	40.579431
3326.358193	1152153.032588	40.584448
3329.735333	1154325.753228	40.589466
3332.531724	1156484.086073	40.594484
3336.219573	1158635.726973	40.599501
3339.556683	1160814.163992	40.604519
3343.009653	1162985.174854	40.609536
3346.567968	1165157.528820	40.614554
3349.883538	1167341.071849	40.619572
3353.086655	1169522.309268	40.624589
3356.669169	1171701.255685	40.629607
3360.035013	1173881.866036	40.634624
3363.238869	1176067.699640	40.639642
3366.428101	1178261.824761	40.644660
3369.925624	1180430.649085	40.649677
3373.152985	1182635.504509	40.654695
3376.397606	1184842.422351	40.659712
3380.346804	1187054.192957	40.664730
3383.586602	1189264.853635	40.669748
3386.879259	1191469.968118	40.674765
3389.859475	1193688.337011	40.679783
3393.102124	1195902.337700	40.684800
3396.560754	1198117.129576	40.689818
3399.727235	1200340.839340	40.694836
3403.195158	1202559.516425	40.699853
3406.612442	1204783.318762	40.704871
3409.688634	1207028.823346	40.709888
3413.537112	1209250.896253	40.714906
3416.937879	1211489.814336	40.719924
3420.179576	1213713.128429	40.724941
3423.502690	1215961.389454	40.729959
3426.558380	1218198.634899	40.734976
3430.953362	1220424.426790	40.739994
3434.225916	1222664.984997	40.745012
3437.549125	1224882.469814	40.750016
3440.985083	1227052.212426	40.755021
3444.051256	1229154.870678	40.760026
3447.255295	1231200.604860	40.765031
3450.331491	1233179.741575	40.770036
3453.595454	1235080.009533	40.775040
3456.475949	1236901.125159	40.780045
3459.092837	1238645.666965	40.785050
3462.431878	1240298.755090	40.790055
3464.831690	1241883.544529	40.795060
3468.064392	1243409.386582	40.800064
3470.465484	1244847.135640	40.805069
3472.845299	1246197.105309	40.810074
3475.457670	1247476.887140	40.815079
3477.528919	1248697.624444	40.820084
3480.016120	1249828.830207	40.825088
3482.207631	1250900.862225	40.830093
3483.835907	1251918.166018	40.835098
3485.921522	1252841.155843	40.840103
3487.602210	1253734.621536	40.845108
3489.233204	1254558.433411	40.850112
3491.085223	1255335.405103	40.855117
3492.289156	1256054.569541	40.860122
3494.182509	1256727.418414	40.865127
3495.526306	1257342.396105	40.870132
3496.812834	1257908.994327	40.875136
3498.383956	1258433.571068	40.880141
3499.634842	1258911.510772	40.885146
3500.886454	1259352.693445	40.890151
3502.066306	1259750.095743	40.895156
3502.942782	1260103.117432	40.900160
3504.365474	1260418.023322	40.905165
3504.947896	1260699.775635	40.910170
3506.054284	1260950.286882	40.915175
3506.613681	1261181.507374	40.920180
3507.597508	1261361.772894	40.925184
3508.537957	1261533.143233	40.930189
3509.302662	1261672.938979	40.935194
3510.221840	1261765.263533	40.940199
3510.758199	1261852.367876	40.945204
3511.296363	1261911.209928	40.950208
3511.704224	1261946.537951	40.955213
3512.191145	1261968.788158	40.960218
3512.967915	1261969.216315	40.965223
3513.227365	1261957.406344	40.970228
3513.706687	1261908.033954	40.975232
3514.386911	1261852.790504	40.980237
3514.367627	1261788.025028	40.985242
3515.050485	1261688.858384	40.990247
3515.291088	1261597.916984	40.995252
3515.510461	1261477.602518	41.000256
3515.966996	1261354.744061	41.005261
3516.491761	1261224.087043	41.010266
3517.047722	1261070.716599	41.015271
3517.367534	1260913.117231	41.020276
3517.493959	1260732.652965	41.025280
3517.605844	1260535.594315	41.030285
3517.870873	1260340.541765	41.035290
3518.353427	1260141.274698	41.040295
3518.350923	1259936.517904	41.045300
3518.840552	1259710.165668	41.050304
3519.229583	1259486.971621	41.055309
3519.337954	1259242.862048	41.060314
3519.506338	1258982.784218	41.065319
3519.800478	1258727.586111	41.070324
3519.665889	1258466.325943	41.075328
3520.020610	1258190.042543	41.080333
3519.733783	1257924.420922	41.085338
3520.021813	1257635.599040	41.090343
3520.234330	1257375.430192	41.095348
3520.296904	1257081.234352	41.100352
3520.508220	1256790.150279	41.105357
3520.260023	1256506.916593	41.110362
3520.681413	1256199.994668	41.115367
3520.685612	1255895.720142	41.120372
3520.753257	1255598.096430	41.125376
3520.800333	1255278.283835	41.130381
3520.984236	1254961.304633	41.135386
3520.663670	1254637.150594	41.140391
3520.805439	1254320.508880	41.145396
3521.146578	1253996.389931	41.150400
3521.261992	1253687.600876	41.155405
3521.330557	1253352.904752	41.160410
3521.357596	1253018.935661	41.165415
3521.378393	1252686.894717	41.170420
3521.387884	1252343.507729	41.175424
3521.421237	1252003.899760	41.180429
3521.447960	1251656.006389	41.185434
3521.568706	1251325.065691	41.190439
3521.734837	1250974.130672	41.195444
3521.591456	1250615.235470	41.200448
3521.554215	1250277.843771	41.205453
3521.041074	1249927.318790	41.210458
3521.574083	1249570.745151	41.215463
3521.761732	1249230.087747	41.220468
3521.496003	1248873.596078	41.225472
3521.673193	1248526.854157	41.230477
3521.667001	1248181.047594	41.235482
3521.697056	1247812.724844	41.240487
3521.791168	1247457.002424	41.245492
3521.592584	1247090.429903	41.250496
3521.867937	1246719.012652	41.255501
3521.793661	1246361.474481	41.260506
3522.061170	1245995.395870	41.265511
3521.709580	1245632.181322	41.270516
3521.770057	1245260.319744	41.275520
3521.885388	1244893.070273	41.280525
3521.824756	1244537.445426	41.285530
3521.751011	1244153.901598	41.290535
3521.814546	1243796.065154	41.295540
3521.710038	1243421.490877	41.300544
3521.751247	1243059.513680	41.305549
3521.341554	1242685.492885	41.310554
3521.631948	1242307.980227	41.315559
3521.532366	1241952.458026	41.320564
3521.453547	1241580.533257	41.325568
3521.897603	1241200.958547	41.330573
3521.598784	1240828.177053	41.335578
3521.699325	1240468.609067	41.340583
3521.649565	1240088.008197	41.345588
3521.393430	1239716.347176	41.350592
3521.445070	1239355.590974	41.355597
3521.208995	1238981.359393	41.360602
3521.079304	1238608.292663	41.365607
3521.385412	1238237.081575	41.370612
3521.027502	1237870.049050	41.375616
3521.467484	1237491.405896	41.380621
3521.545603	1237124.899109	41.385626
3521.360554	1236756.825940	41.390631
3521.191968	1236374.939905	41.395636
3521.450534	1236005.062499	41.400640
3521.464651	1235638.644589	41.405645
3521.467452	1235269.407424	41.410650
3521.273607	1234877.351944	41.415655
3521.504923	1234503.922224	41.420660
3521.039708	1234127.970797	41.425664
3521.485647	1233749.791400	41.430669
3521.091653	1233377.872304	41.435674
3521.236576	1233010.962679	41.440679
3520.856646	1232631.158139	41.445684
3520.845511	1232243.434969	41.450688
3520.823219	1231867.708489	41.455693
3520.744597	1231510.887121	41.460698
3521.010963	1231127.227610	41.465703
3520.993203	1230752.163365	41.470708
3520.678648	1230394.090058	41.475712
3520.946092	1230012.397174	41.480717
3520.402918	1229644.610719	41.485722
3520.580393	1229275.186681	41.490727
3520.398069	1228900.385398	41.495732
3520.445862	1228531.394823	41.500736
3520.412035	1228160.058773	41.505741
3520.417608	1227807.906476	41.510746
3520.365011	1227430.642908	41.515751
3520.589302	1227069.167033	41.520756
3520.224766	1226705.989502	41.525760
3520.665636	1226328.935943	41.530765
3520.276600	1225965.242827	41.535770
3520.451598	1225595.644344	41.540775
3520.369019	1225240.901754	41.545780
3520.207515	1224865.985422	41.550784
3520.532012	1224501.603184	41.555789
3519.903358	1224141.926212	41.560794
3520.127377	1223756.968770	41.565799
3520.353171	1223398.778983	41.570804
3519.965023	1223037.023385	41.575808
3519.980422	1222672.280700	41.580813
3519.661101	1222307.380183	41.585818
3519.890356	1221946.565952	41.590823
3519.819517	1221584.841514	41.595828
3520.043680	1221221.267981	41.600832
3519.925572	1220870.616246	41.605837
3519.714204	1220504.821250	41.610842
3519.616855	1220130.572523	41.615847
3519.723319	1219774.482769	41.620852
3519.673388	1219415.123370	41.625856
3520.038050	1219058.941049	41.630861
3519.689189	1218699.860742	41.635866
3519.548231	1218332.122324	41.640871
3519.347607	1217974.274913	41.645876
3519.459234	1217622.146427	41.650880
3519.327097	1217269.192414	41.655885
3519.410177	1216902.061729	41.660890
3519.523427	1216542.566258	41.665895
3519.579846	1216186.046861	41.670900
3519.495766	1215831.302337	41.675904
3519.307052	1215459.998203	41.680909
3519.207421	1215117.363542	41.685914
3519.196627	1214767.770179	41.690919
3519.207855	1214408.702266	41.695924
3519.063092	1214056.556813	41.700928
3518.972141	1213695.865384	41.705933
3518.518951	1213338.108303	41.710938
3518.767103	1213001.355309	41.715943
3519.004719	1212653.073169	41.720948
3518.735943	1212302.604930	41.725952
3518.779717	1211957.395199	41.730957
3518.549143	1211620.723621	41.735962
3518.961721	1211257.718197	41.740967
3518.976468	1210915.250625	41.745972
3518.542701	1210559.167669	41.750976
3518.554549	1210215.530446	41.755981
3518.562741	1209870.560091	41.760986
3518.828087	1209522.809030	41.765991
3518.461589	1209182.628812	41.770996
3518.518193	1208831.400823	41.776000
3518.636376	1208485.382598	41.781005
3518.649218	1208135.986960	41.786010
3518.607542	1207788.355915	41.791015
3518.532479	1207451.384228	41.796020
3518.295732	1207104.113506	41.801024
3518.264137	1206753.319492	41.806029
3518.053055	1206416.583150	41.811034
3518.171072	1206067.872226	41.816039
3518.381337	1205727.648489	41.821044
3518.275785	1205388.765980	41.826048
3518.515525	1205045.774856	41.831053
3518.209316	1204706.880323	41.836058
3518.214377	1204352.261166	41.841063
3518.155974	1204017.216424	41.846068
3517.854029	1203665.974469	41.851072
3518.256646	1203334.745942	41.856077
3518.117161	1202996.554584	41.861082
3518.015854	1202646.990963	41.866087
3517.854099	1202319.633619	41.871092
3517.971901	1201970.925441	41.876096
3517.868239	1201635.076306	41.881101
3517.817059	1201297.602405	41.886106
3517.853490	1200968.438357	41.891111
3517.956275	1200628.081717	41.896116
3517.787128	1200291.311443	41.901120
3517.850552	1199957.576159	41.906125
3517.629242	1199610.170583	41.911130
3517.586314	1199265.432683	41.916135
3517.412501	1198944.898118	41.921140
3516.935370	1198615.292685	41.926144
3517.109918	1198287.623044	41.931149
3517.210177	1197956.660543	41.936154
3516.879908	1197632.316543	41.941159
3516.921788	1197309.955444	41.946164
3516.807463	1196989.946205	41.951168
3517.101887	1196670.788346	41.956173
3516.922167	1196350.374694	41.961178
3517.130508	1196011.103097	41.966183
3517.155431	1195696.435041	41.971188
3516.848383	1195368.658922	41.976192
3516.956422	1195048.492426	41.981197
3516.689153	1194730.809095	41.986202
3516.686987	1194410.715025	41.991207
3516.468717	1194093.735555	41.996212
3516.315882	1193766.301645	42.001216
3516.377674	1193464.826685	42.006221
3516.257098	1193153.314416	42.011226
3516.196459	1192833.132043	42.016231
3515.895621	1192524.429339	42.021236
3516.132312	1192212.237803	42.026240
3516.234300	1191904.840791	42.031245
3516.100173	1191595.209534	42.036250
3516.250831	1191284.103453	42.041255
3515.941844	1190986.115085	42.046260
3515.876598	1190677.169124	42.051264
3516.196551	1190367.107537	42.056269
3515.987801	1190068.767807	42.061274
3515.799672	1189762.418779	42.066279
3515.886990	1189450.742781	42.071284
3515.805783	1189144.057515	42.076288
3516.017712	1188829.785670	42.081293
3515.722482	1188543.686292	42.086298
3515.765048	1188238.619044	42.091303
3515.281697	1187943.680293	42.096308
3515.075541	1187637.490332	42.101312
3515.360749	1187342.108631	42.106317
3515.587218	1187045.403270	42.111322
3515.545993	1186750.793849	42.116327
3515.550918	1186454.655342	42.121332
3515.507347	1186149.855277	42.126336
3515.407658	1185844.670283	42.131341
3515.407661	1185569.080069	42.136346
3515.427242	1185269.391100	42.141351
3515.630621	1184955.637844	42.146356
3515.395332	1184664.140068	42.151360
3515.318198	1184374.199240	42.156365
3515.297650	1184073.789131	42.161370
3515.295007	1183781.921136	42.166375
3515.114136	1183490.442451	42.171380
3514.926238	1183192.267163	42.176384
3515.156072	1182895.699893	42.181389
3515.113853	1182610.454204	42.186394
3515.269317	1182319.230734	42.191399
3515.271179	1182028.392711	42.196404
3514.910847	1181729.032175	42.201408
3515.015805	1181443.321538	42.206413
3515.069905	1181153.837917	42.211418
3515.030633	1180858.893052	42.216423
3514.937033	1180584.088753	42.221428
3514.530715	1180292.561592	42.226432
3514.749360	1179996.583690	42.231437
3514.569865	1179725.608722	42.236442
3514.787298	1179422.629972	42.241447
3514.608050	1179136.556657	42.246452
3514.350593	1178849.538640	42.251456
3514.640485	1178558.835484	42.256461
3514.437425	1178289.861624	42.261466
3514.748685	1178019.470371	42.266471
3514.694731	1177722.560025	42.271476
3514.369035	1177430.293682	42.276480
3514.606290	1177148.658530	42.281485
3514.327117	1176881.131715	42.286490
3514.341521	1176597.147942	42.291495
3514.310867	1176310.423456	42.296500
3513.835723	1176042.037689	42.301504
3514.458270	1175768.274184	42.306509
3514.199262	1175495.395414	42.311514
3514.520339	1175212.416471	42.316519
3514.552974	1174929.281145	42.321524
3513.895607	1174654.915849	42.326528
3514.075787	1174372.385744	42.331533
3514.067042	1174106.462706	42.336538
3513.919977	1173823.014005	42.341543
3513.807766	1173555.477221	42.346548
3514.101554	1173292.573995	42.351552
3513.915427	1173013.990428	42.356557
3513.581025	1172738.528060	42.361562
3513.589870	1172465.917842	42.366567
3513.968578	1172198.041909	42.371572
3513.360879	1171938.425137	42.376576
3513.510174	1171656.224355	42.381581
3513.489264	1171396.955539	42.386586
3513.424784	1171134.002441	42.391591
3513.567012	1170867.417614	42.396596
3513.480238	1170610.101398	42.401600
3513.591417	1170342.457211	42.406605
3513.726461	1170079.229411	42.411610
3513.530356	1169806.608253	42.416615
3513.375642	1169538.683592	42.421620
3513.243982	1169281.969726	42.426624
3513.493406	1169015.272623	42.431629
3513.260910	1168755.907397	42.436634
3513.092328	1168496.235649	42.441639
3513.192535	1168238.016714	42.446644
3513.221344	1167975.738463	42.451648
3513.286797	1167716.838834	42.456653
3512.613066	1167467.958917	42.461658
3513.060837	1167205.384215	42.466663
3512.927573	1166951.104638	42.471668
3512.696609	1166704.475371	42.476672
3512.840992	1166447.387892	42.481677
3512.867383	1166200.881294	42.486682
3513.005037	1165941.881840	42.491687
3512.885539	1165683.761698	42.496692
3512.828503	1165435.061058	42.501696
3512.705329	1165180.221549	42.506701
3512.589880	1164929.712332	42.511706
3512.473534	1164675.980343	42.516711
3512.907860	1164444.245096	42.521716
3512.135189	1164186.914194	42.526720
3512.593566	1163940.985521	42.531725
3512.471941	1163697.218866	42.536730
3512.354560	1163451.928782	42.541735
3512.343440	1163204.342533	42.546740
3512.193791	1162969.331880	42.551744
3512.576592	1162716.839750	42.556749
3512.317803	1162471.149109	42.561754
3512.317542	1162223.798149	42.566759
3512.261701	1161987.688682	42.571764
3511.951589	1161742.539238	42.576768
3512.232918	1161493.595558	42.581773
3512.228001	1161254.609779	42.586778
3512.008238	1161033.887912	42.591783
3511.840237	1160781.204211	42.596788
3511.623900	1160545.150684	42.601792
3511.830901	1160318.185015	42.606797
3512.231553	1160074.636321	42.611802
3511.699228	1159836.996077	42.616807
3511.634984	1159595.297686	42.621812
3511.699178	1159377.578822	42.626816
3511.984372	1159133.249164	42.631821
3512.131048	1158899.519783	42.636826
3511.813700	1158669.921946	42.641831
3511.756260	1158431.005211	42.646836
3511.829244	1158193.096235	42.651840
3511.760857	1157971.747754	42.656845
3511.603266	1157743.217776	42.661850
3511.492073	1157487.907378	42.666855
3511.710906	1157262.320667	42.671860
3511.339383	1157042.496091	42.676864
3511.467297	1156809.055025	42.681869
3511.583056	1156584.212812	42.686874
3511.154657	1156368.436529	42.691879
3511.173031	1156130.159310	42.696884
3510.907924	1155914.999656	42.701888
3511.234593	1155695.192892	42.706893
3511.461400	1155470.284726	42.711898
3511.269230	1155249.977166	42.716903
3511.361268	1155029.992016	42.721908
3511.171990	1154804.650834	42.726912
3511.240909	1154579.446711	42.731917
3511.357408	1154354.792859	42.736922
3511.106633	1154136.246148	42.741927
3511.418394	1153903.686669	42.746932
3510.939862	1153677.493119	42.751936
3511.192019	1153464.892455	42.756941
3510.993184	1153255.670044	42.761946
3511.025802	1153034.096877	42.766951
3511.214103	1152799.142696	42.771956
3510.861392	1152600.236721	42.776960
3511.011328	1152375.966144	42.781965
3511.047035	1152156.911374	42.786970
3510.476234	1151935.391329	42.791975
3510.782484	1151708.889218	42.796980
3510.373391	1151503.797369	42.801985
3510.568095	1151283.354603	42.806989
3510.551008	1151086.703158	42.811994
3510.324900	1150873.981939	42.816999
3510.488050	1150661.756168	42.822004
3510.349571	1150475.612631	42.827009
3510.250619	1150264.266268	42.832013
3510.372157	1150048.992319	42.837018
3510.068878	1149843.913099	42.842023
3510.454638	1149635.018736	42.847028
3509.970613	1149435.162412	42.852033
3510.261479	1149226.078050	42.857037
3510.174080	1149034.855195	42.862042
3510.393206	1148823.872291	42.867047
3510.278872	1148623.071770	42.872052
3509.874814	1148427.047893	42.877057
3510.178380	1148215.079415	42.882061
3510.153387	1148010.451441	42.887066
3509.682762	1147814.510494	42.892071
3509.948371	1147608.682166	42.897076
3509.907898	1147408.202211	42.902081
3509.773700	1147217.868679	42.907085
3509.842958	1147023.894021	42.912090
3509.574468	1146829.588817	42.917095
3509.882686	1146629.874712	42.922100
3509.418883	1146441.273200	42.927105
3509.529094	1146244.799221	42.932109
3509.577190	1146056.383964	42.937114
3509.965770	1145870.370122	42.942119
3509.860566	1145671.446078	42.947124
3509.724764	1145478.964925	42.952129
3509.895953	1145273.535030	42.957133
3510.145378	1145086.663422	42.962138
3509.856462	1144897.788381	42.967143
3510.008091	1144693.855888	42.972148
3509.661060	1144494.548153	42.977153
3509.694236	1144302.565117	42.982157
3509.579680	1144108.324021	42.987162
3509.600651	1143909.312839	42.992167
3509.835056	1143715.094636	42.997172
3509.639610	1143528.241193	43.002177
3509.472642	1143328.670188	43.007181
3509.179398	1143142.103670	43.012186
3509.541274	1142954.664036	43.017191
3509.554405	1142759.024716	43.022196
3509.213283	1142583.162502	43.027201
3509.282948	1142397.078946	43.032205
3509.208286	1142217.651624	43.037210
3508.847058	1142029.065326	43.042215
3509.222794	1141840.256083	43.047220
3508.976440	1141661.502121	43.052225
3509.197431	1141481.716590	43.057229
3509.269225	1141301.570088	43.062234
3508.992479	1141121.095407	43.067239
3509.286013	1140932.172452	43.072244
3509.188664	1140750.801806	43.077249
3509.411831	1140565.102897	43.082253
3509.285590	1140382.680801	43.087258
3509.290946	1140193.589206	43.092263
3509.031149	1140005.103824	43.097268
3508.905469	1139836.230997	43.102273
3509.098311	1139652.307904	43.107277
3508.925017	1139478.687072	43.112282
3508.683038	1139299.852626	43.117287
3508.730380	1139120.110407	43.122292
3508.696272	1138943.697062	43.127297
3508.893019	1138769.232822	43.132301
3508.811950	1138593.954425	43.137306
3508.354362	1138421.484656	43.142311
3509.076509	1138244.069276	43.147316
3508.915402	1138079.797082	43.152321
3508.975738	1137889.854866	43.157325
3508.873839	1137719.961459	43.162330
3508.336514	1137541.685850	43.167335
3508.734258	1137361.731366	43.172340
3508.439333	1137197.358933	43.177345
3508.416533	1137020.499982	43.182349
3508.442566	1136859.956606	43.187354
3508.337780	1136694.113174	43.192359
3508.536844	1136511.883980	43.197364
3508.561175	1136355.882993	43.202369
3508.376568	1136188.612685	43.207373
3508.278657	1136018.569161	43.212378
3508.321451	1135859.132185	43.217383
3508.583557	1135683.796016	43.222388
3508.460788	1135525.895656	43.227393
3508.183477	1135347.598410	43.232397
3508.418167	1135178.137942	43.237402
3508.151855	1135028.983576	43.242407
3508.428691	1134853.902490	43.247412
3508.013792	1134687.762494	43.252417
3508.264393	1134523.312327	43.257421
3508.029096	1134371.664885	43.262426
3507.905073	1134203.562162	43.267431
3508.064567	1134031.227887	43.272436
3508.230348	1133886.339770	43.277441
3508.024010	1133716.335340	43.282445
3508.018607	1133550.092301	43.287450
3507.889891	1133395.644488	43.292455
3508.089639	1133243.133164	43.297460
3507.704921	1133085.583379	43.302465
3507.808963	1132916.452296	43.307469
3508.026194	1132757.083464	43.312474
3507.700554	1132606.540646	43.317479
3507.791751	1132448.038440	43.322484
3507.892890	1132297.701640	43.327489
3507.840602	1132141.969534	43.332493
3507.907412	1131979.846502	43.337498
3507.776266	1131830.389980	43.342503
3507.785235	1131659.714111	43.347508
3507.483895	1131512.272344	43.352513
3507.465639	1131360.598229	43.357517
3507.766601	1131206.871377	43.362522
3507.218167	1131060.503215	43.367527
3507.605022	1130912.741398	43.372532
3507.623148	1130764.180777	43.377537
3507.845538	1130610.734787	43.382541
3507.645669	1130453.836940	43.387546
3507.139041	1130311.528570	43.392551
3507.368798	1130153.790670	43.397556
3507.213569	1130020.542278	43.402561
3507.459795	1129872.204370	43.407565
3507.594649	1129715.609883	43.412570
3507.189127	1129571.268657	43.417575
3507.522905	1129429.653910	43.422580
3507.140933	1129290.530132	43.427585
3507.088529	1129136.611530	43.432589
3507.280687	1129005.086965	43.437594
3507.040848	1128852.807376	43.442599
3507.572149	1128705.721172	43.447604
3507.122383	1128568.871727	43.452609
3507.164713	1128419.956421	43.457613
3507.289478	1128274.066333	43.462618
3507.194314	1128138.478717	43.467623
3507.410216	1127987.335552	43.472628
3507.227305	1127836.158683	43.477633
3507.497972	1127690.704094	43.482637
3507.388285	1127547.020075	43.487642
3507.195958	1127402.584927	43.492647
3507.654146	1127251.761431	43.497652
3507.303573	1127116.760539	43.502657
3506.985580	1126957.591486	43.507661
3507.069881	1126812.809444	43.512666
3506.844109	1126675.208609	43.517671
3507.090924	1126542.663047	43.522676
3506.678102	1126405.466546	43.527681
3506.938504	1126266.728714	43.532685
3507.110505	1126134.660975	43.537690
3506.539312	1126001.856168	43.542695
3506.786051	1125871.386859	43.547700
3506.979839	1125728.555183	43.552705
3506.526916	1125594.864515	43.557709
3506.826202	1125464.281456	43.562714
3506.881594	1125329.929576	43.567719
3507.196400	1125186.302294	43.572724
3506.672916	1125059.079835	43.577729
3506.654766	1124916.737077	43.582733
3506.771940	1124786.928654	43.587738
3506.418862	1124653.768872	43.592743
3506.794525	1124520.009949	43.597748
3506.785699	1124388.404556	43.602753
3506.710315	1124266.037782	43.607757
3506.654803	1124130.246500	43.612762
3506.581244	1123989.410792	43.617767
3506.415018	1123845.350802	43.622772
3506.613821	1123730.254778	43.627777
3506.521579	1123594.170386	43.632781
3506.570198	1123469.099994	43.637786
3506.341169	1123338.076037	43.642791
3506.810786	1123194.464847	43.647796
3506.599363	1123085.514195	43.652801
3506.306250	1122950.493511	43.657805
3506.336962	1122824.744665	43.662810
3506.294298	1122705.477981	43.667815
3506.379416	1122573.526797	43.672820
3506.266673	1122450.838983	43.677825
3506.569465	1122327.699120	43.682829
3506.568607	1122198.418387	43.687834
3506.336920	1122079.930472	43.692839
3506.685622	1121941.541677	43.697844
3506.169124	1121812.907768	43.702849
3506.438476	1121687.759309	43.707853
3506.551938	1121550.160802	43.712858
3506.084339	1121424.651492	43.717863
3506.253757	1121300.748219	43.722868
3506.552927	1121187.675653	43.727873
3506.202339	1121057.948830	43.732877
3506.353724	1120935.849270	43.737882
3506.100230	1120805.909891	43.742887
3506.312319	1120689.984375	43.747892
3506.149515	1120561.357301	43.752897
3506.469183	1120427.695596	43.757901
3506.532954	1120306.167482	43.762906
3506.052183	1120192.440448	43.767911
3506.404575	1120052.383129	43.772916
3505.935868	1119941.315453	43.777921
3506.048319	1119820.625457	43.782925
3506.267247	1119701.534370	43.787930
3505.999036	1119586.045011	43.792935
3506.201380	1119456.092995	43.797940
3506.165406	1119336.178510	43.802945
3505.894781	1119221.729449	43.807949
3506.350143	1119096.108692	43.812954
3505.874919	1118984.450672	43.817959
3505.977253	1118864.693357	43.822964
3505.946410	1118754.672034	43.827969
3505.937551	1118635.880533	43.832973
3505.967071	1118509.649298	43.837978
3505.931427	1118389.237204	43.842983
3506.248037	1118275.909685	43.847988
3506.202081	1118168.832196	43.852993
3505.955591	1118040.062987	43.857997
3505.895145	1117917.643598	43.863002
3505.694791	1117805.344029	43.868007
3505.436635	1117682.475427	43.873012
3505.460905	1117572.706573	43.878017
3505.462742	1117460.938177	43.883021
3505.794384	1117350.351863	43.888026
3505.619077	1117243.944185	43.893031
3505.765155	1117131.192263	43.898036
3505.705609	1117024.094114	43.903041
3505.489297	1116911.111363	43.908045
3506.110300	1116797.225953	43.913050
3505.905197	1116688.525019	43.918055
3506.091610	1116563.079741	43.923060
3505.502581	1116459.297734	43.928065
3505.460905	1116340.174788	43.933069
3505.826649	1116234.515689	43.938074
3505.356909	1116126.990623	43.943079
3505.353831	1116010.236703	43.948084
3505.334384	1115912.068931	43.953089
3505.354220	1115808.364654	43.958093
3505.662077	1115689.646251	43.963098
3505.093537	1115591.467721	43.968103
3505.821123	1115471.817504	43.973108
3505.679192	1115358.027178	43.978113
3505.491319	1115256.920147	43.983117
3505.655549	1115147.745821	43.988122
3505.386868	1115059.803381	43.993127
3505.159619	1114935.913388	43.998132
3505.277527	1114833.127390	44.003137
3505.195881	1114731.706959	44.008141
3505.431592	1114615.646002	44.013146
3505.188741	1114525.211807	44.018151
3505.407335	1114413.820828	44.023156
3505.432163	1114321.527665	44.028161
3505.241035	1114198.854120	44.033165
3505.506725	1114098.222591	44.038170
3505.427560	1114008.420134	44.043175
3505.297661	1113891.450258	44.048180
3505.216944	1113786.007146	44.053185
3505.082530	1113682.096440	44.058189
3505.464663	1113573.521649	44.063194
3505.079006	1113474.702075	44.068199
3505.163970	1113365.885957	44.073204
3505.108958	1113281.693468	44.078209
3505.031839	1113177.668195	44.083213
3505.021479	1113078.493426	44.088218
3504.934911	1112984.860529	44.093223
3505.370422	1112885.704131	44.098228
3504.678775	1112777.766921	44.103233
3504.996838	1112676.623269	44.108237
3505.133990	1112590.480882	44.113242
3504.827725	1112486.861442	44.118247
3504.990867	1112383.258067	44.123252
3504.973548	1112297.899429	44.128257
3504.734275	1112193.214139	44.133261
3505.095844	1112103.688725	44.138266
3504.978552	1112013.096103	44.143271
3504.986937	1111904.167581	44.148276
3504.754680	1111801.285784	44.153281
3504.952313	1111709.873093	44.158285
3505.257642	1111620.825833	44.163290
3504.623235	1111527.257731	44.168295
3504.780722	1111427.643253	44.173300
3504.718656	1111334.836065	44.178305
3504.513404	1111250.254873	44.183309
3504.453041	1111157.158147	44.188314
3504.656800	1111069.549435	44.193319
3504.529299	1110979.704245	44.198324
3504.819446	1110886.831308	44.203329
3504.573168	1110797.670449	44.208333
3505.156348	1110707.703666	44.213338
3504.454039	1110619.855225	44.218343
3504.633302	1110516.690222	44.223348
3504.673472	1110447.607534	44.228353
3504.484703	1110349.175003	44.233357
3504.931256	1110249.968142	44.238362
3504.519778	1110170.651635	44.243367
3504.570883	1110077.804089	44.248372
3504.717626	1109991.523023	44.253377
3504.676263	1109904.317358	44.258381
3504.680070	1109809.850843	44.263386
3504.536198	1109738.594666	44.268391
3504.553540	1109635.725689	44.273396
3504.656226	1109543.242110	44.278401
3504.134338	1109464.696766	44.283405
3504.351511	1109383.261122	44.288410
3503.972841	1109303.640119	44.293415
3504.195245	1109207.409272	44.298420
3504.450723	1109133.693509	44.303425
3504.195459	1109051.280882	44.308429
3504.551110	1108972.679252	44.313434
3504.371842	1108889.297266	44.318439
3504.465467	1108789.930725	44.323444
3504.547395	1108706.980090	44.328449
3504.300547	1108627.518238	44.333453
3504.458760	1108538.253259	44.338458
3504.277687	1108460.877870	44.343463
3504.486359	1108372.365388	44.348468
3504.465519	1108290.379719	44.353473
3504.284431	1108212.046272	44.358477
3504.348415	1108126.512505	44.363482
3503.867682	1108039.921661	44.368487
3504.131701	1107960.461265	44.373492
3504.043797	1107880.962200	44.378497
3504.171360	1107797.894575	44.383501
3504.111268	1107721.729563	44.388506
3504.308599	1107644.184644	44.393511
3504.456868	1107560.823571	44.398516
3504.392026	1107489.238176	44.403521
3504.053848	1107412.064494	44.408525
3504.285504	1107317.516664	44.413530
3504.156126	1107239.351462	44.418535
3504.492189	1107155.093978	44.423540
3504.252636	1107080.285996	44.428545
3503.844248	1106996.625984	44.433549
3504.165742	1106922.009813	44.438554
3504.224349	1106860.324830	44.443559
3504.268634	1106770.285497	44.448564
3504.503101	1106684.891688	44.453569
3504.078240	1106605.906659	44.458573
3504.002825	1106516.646621	44.463578
3503.674430	1106457.694186	44.468583
3503.830638	1106374.408913	44.473588
3503.399005	1106299.144291	44.478593
3503.622426	1106234.083069	44.483597
3503.785473	1106153.848763	44.488602
3503.532386	1106088.100368	44.493607
3503.904210	1106032.751951	44.498612
3503.709589	1105948.753969	44.503617
3503.929704	1105879.869431	44.508621
3504.029532	1105811.672267	44.513626
3504.039818	1105738.141363	44.518631
3503.758732	1105658.545785	44.523636
3504.194241	1105591.436484	44.528641
3504.139411	1105524.311609	44.533645
3504.234552	1105442.931932	44.538650
3503.586915	1105368.453853	44.543655
3503.641576	1105305.223706	44.548660
3504.230168	1105228.630072	44.553665
3503.549904	1105146.991619	44.558669
3503.938362	1105073.962388	44.563674
3503.804873	1105004.647372	44.568679
3503.663779	1104923.298751	44.573684
3503.893598	1104860.321059	44.578689
3503.744823	1104792.247442	44.583693
3504.011629	1104705.288764	44.588698
3503.795720	1104644.387701	44.593703
3503.934187	1104571.297322	44.598708
3503.909980	1104496.704499	44.603713
3503.741718	1104417.263017	44.608717
3503.905936	1104360.116803	44.613722
3503.986959	1104283.115748	44.618727
3503.636001	1104208.954831	44.623732
3503.843996	1104134.223227	44.628737
3503.903717	1104067.252371	44.633741
3503.963747	1103995.886521	44.638746
3503.864203	1103917.668169	44.643751
3503.707328	1103840.604447	44.648756
3503.992576	1103780.661877	44.653761
3504.053967	1103698.401660	44.658765
3503.818300	1103623.927112	44.663770
3503.817166	1103556.577811	44.668775
3503.696416	1103494.788289	44.673780
3503.513458	1103421.257589	44.678785
3503.808763	1103357.200677	44.683789
3503.933574	1103284.190633	44.688794
3503.754268	1103214.286905	44.693799
3503.917958	1103129.803790	44.698804
3503.892125	1103068.471447	44.703809
3504.019903	1102990.966533	44.708813
3504.028610	1102910.995988	44.713818
3503.941127	1102850.817844	44.718823
3503.830106	1102771.342669	44.723828
3503.710005	1102694.829783	44.728833
3503.782361	1102638.158188	44.733837
3503.724398	1102561.059880	44.738842
3503.323693	1102487.361201	44.743847
3503.671264	1102420.991346	44.748852
3503.602662	1102369.499954	44.753857
3503.514073	1102294.313936	44.758861
3503.948312	1102224.869657	44.763866
3503.686178	1102162.037033	44.768871
3503.787682	1102084.427865	44.773876
3503.446592	1102018.548713	44.778881
3503.246969	1101952.932137	44.783885
3503.546755	1101880.447638	44.788890
3503.452380	1101828.095267	44.793895
3503.672330	1101749.315021	44.798900
3503.632113	1101695.710113	44.803905
3503.453004	1101632.379817	44.808909
3503.868177	1101567.612962	44.813914
3503.657516	1101503.999654	44.818919
3503.647150	1101436.243119	44.823924
3503.520276	1101370.320765	44.828929
3503.218174	1101292.479967	44.833933
3503.474355	1101219.324770	44.838938
3503.165865	1101167.192394	44.843943
3503.462469	1101106.071355	44.848948
3503.556967	1101042.020039	44.853953
3503.495421	1100981.147724	44.858957
3503.737824	1100922.327395	44.863962
3503.439806	1100848.111499	44.868967
3503.445848	1100781.013095	44.873972
3503.240794	1100714.139788	44.878977
3503.242926	1100667.686363	44.883981
3503.118404	1100597.548519	44.888986
3503.244030	1100539.985855	44.893991
3503.466413	1100483.362507	44.898996
3503.486570	1100427.918920	44.904001
3503.189844	1100369.085770	44.909005
3503.346645	1100291.441713	44.914010
3503.441791	1100240.476571	44.919015
3503.126465	1100177.438401	44.924020
3503.220870	1100107.640503	44.929025
3503.150171	1100055.075842	44.934029
3503.324444	1099987.270708	44.939034
3503.371949	1099930.957158	44.944039
3503.416414	1099873.687549	44.949044
3503.367006	1099812.417666	44.954049
3503.159129	1099757.673941	44.959053
3503.257519	1099698.194806	44.964058
3503.456767	1099648.162933	44.969063
3503.217591	1099578.030726	44.974068
3503.106555	1099522.790657	44.979073
3502.930440	1099468.994807	44.984077
3503.396069	1099407.922325	44.989082
3503.108415	1099353.665669	44.994087
3503.094418	1099290.758726	44.999092
3503.226618	1099235.666876	45.004097
3502.904558	1099175.964412	45.009101
3503.375419	1099120.050731	45.014106
3503.180237	1099062.429548	45.019111
3503.501366	1099006.348129	45.024116
3503.768260	1098935.933010	45.029121
3503.313864	1098880.456079	45.034125
3503.120896	1098810.975601	45.039130
3503.143539	1098755.036351	45.044135
3503.111542	1098705.990012	45.049140
3503.237091	1098648.215968	45.054145
3503.204270	1098584.060852	45.059149
3503.348589	1098519.110830	45.064154
3502.854877	1098477.405662	45.069159
3502.981388	1098409.014860	45.074164
3503.361035	1098355.212006	45.079169
3503.358530	1098308.260930	45.084173
3503.210312	1098237.713834	45.089178
3502.897676	1098175.512473	45.094183
3502.930154	1098122.338244	45.099188
3502.835825	1098074.826492	45.104193
3502.889565	1098021.169621	45.109197
3503.086254	1097961.272659	45.114202
3502.836825	1097911.585502	45.119207
3502.972695	1097844.716131	45.124212
3503.298591	1097794.168077	45.129217
3502.993382	1097749.174677	45.134221
3503.055169	1097700.008127	45.139226
3503.266906	1097644.791328	45.144231
3503.094616	1097581.603648	45.149236
3503.058464	1097524.131137	45.154241
3503.147977	1097489.877739	45.159245
3503.260494	1097417.172923	45.164250
3503.450745	1097369.321179	45.169255
3502.748039	1097301.435500	45.174260
3503.175839	1097245.987762	45.179265
3502.876374	1097200.797560	45.184269
3503.076932	1097144.525407	45.189274
3503.076186	1097093.928963	45.194279
3502.995969	1097041.719130	45.199284
3503.315667	1096970.791490	45.204289
3502.869133	1096920.745088	45.209293
3502.885936	1096868.421953	45.214298
3502.851291	1096827.967535	45.219303
3502.962396	1096763.288846	45.224308
3503.122413	1096713.810197	45.229313
3502.708947	1096680.399737	45.234317
3502.937495	1096615.412977	45.239322
3502.932720	1096560.125113	45.244327
3502.871813	1096514.315944	45.249332
3503.162007	1096462.900428	45.254337
3502.588995	1096407.226298	45.259341
3503.027633	1096351.384980	45.264346
3503.004269	1096313.794643	45.269351
3502.850815	1096254.127767	45.274356
3502.903809	1096201.600900	45.279361
3502.847415	1096159.423143	45.284365
3502.981044	1096100.855250	45.289370
3502.833038	1096050.273296	45.294375
3502.706878	1096009.445168	45.299380
3502.831885	1095947.911406	45.304385
3502.470730	1095911.139236	45.309389
3503.126061	1095864.249928	45.314394
3502.854062	1095810.816111	45.319399
3502.889674	1095759.435843	45.324404
3503.240388	1095712.499722	45.329409
3502.672347	1095663.035702	45.334413
3502.639587	1095608.603768	45.339418
3502.649665	1095562.870522	45.344423
3502.705324	1095522.008770	45.349428
3502.631386	1095471.409203	45.354433
3502.318039	1095423.049139	45.359437
3502.506455	1095370.778932	45.364442
3502.405385	1095343.623419	45.369447
3502.329023	1095296.371320	45.374452
3502.661836	1095248.094629	45.379457
3502.554993	1095205.152308	45.384461
3502.580466	1095155.394532	45.389466
3502.763584	1095112.786447	45.394471
3502.638888	1095071.376907	45.399476
3502.685012	1095020.753353	45.404481
3502.483329	1094978.877370	45.409485
3502.625514	1094934.169577	45.414490
3502.715170	1094887.269302	45.419495
3502.358792	1094849.149522	45.424500
3503.020431	1094789.427934	45.429505
3502.587368	1094757.252734	45.434509
3502.823357	1094708.795810	45.439514
3502.565558	1094663.290460	45.444519
3502.763421	1094622.876947	45.449524
3502.661794	1094563.852721	45.454529
3502.677047	1094524.999612	45.459533
3502.478464	1094468.286915	45.464538
3502.832895	1094432.726530	45.469543
3502.751441	1094387.955367	45.474548
3502.949220	1094330.984565	45.479553
3502.307934	1094287.166027	45.484557
3502.586702	1094241.281669	45.489562
3502.643589	1094201.175320	45.494567
3502.459416	1094156.323461	45.499572
3502.418585	1094111.830419	45.504577
3502.497779	1094079.471118	45.509581
3502.564903	1094031.705848	45.514586
3502.563060	1093981.463280	45.519591
3502.505538	1093947.211676	45.524596
3502.732824	1093893.293876	45.529601
3502.456510	1093854.579679	45.534605
3502.712775	1093805.824230	45.539610
3502.366306	1093773.628911	45.544615
3502.742881	1093720.546151	45.549620
3502.691040	1093676.051342	45.554625
3502.191439	1093640.339296	45.559629
3502.310569	1093596.868460	45.564634
3502.191454	1093554.202185	45.569639
3502.553913	1093514.327552	45.574644
3502.650325	1093475.836388	45.579649
3502.432218	1093431.366952	45.584653
3502.636426	1093387.880429	45.589658
3502.740333	1093349.482845	45.594663
3502.142869	1093310.913361	45.599668
3502.566851	1093258.296835	45.604673
3502.128022	1093234.536359	45.609677
3502.236902	1093179.769530	45.614682
3502.447412	1093143.745820	45.619687
3502.635653	1093103.513996	45.624692
3502.836203	1093059.355422	45.629697
3502.607566	1093017.755853	45.634701
3502.387124	1092972.900162	45.639706
3502.637043	1092931.795432	45.644711
3502.325889	1092884.369508	45.649716
3502.958399	1092831.810223	45.654721
3502.441388	1092807.103527	45.659725
3502.534030	1092757.312654	45.664730
3502.535082	1092707.919304	45.669735
3502.214950	1092664.609059	45.674740
3502.382781	1092627.823154	45.679745
3502.337906	1092601.889056	45.684749
3502.146331	1092539.794354	45.689754
3502.756272	1092506.380979	45.694759
3502.264325	1092470.851401	45.699764
3502.639286	1092430.679561	45.704769
3502.137261	1092396.682817	45.709773
3502.566394	1092356.214316	45.714778
3502.419509	1092310.479451	45.719783
3502.316665	1092277.182060	45.724788
3502.595026	1092228.313056	45.729793
3502.503147	1092192.141364	45.734797
3502.298179	1092154.264849	45.739802
3502.416384	1092113.175609	45.744807
3502.079299	1092069.384722	45.749812
3502.338349	1092030.473568	45.754817
3502.400859	1091970.723893	45.759821
3502.598604	1091875.528115	45.764826
3502.559578	1091710.861762	45.769831
3502.173866	1091481.332393	45.774836
3502.084698	1091208.465457	45.779841
3502.185197	1090874.269870	45.784845
3501.705550	1090471.391550	45.789850
3502.243586	1089995.050749	45.794855
3502.262914	1089467.510916	45.799860
3501.857783	1088873.223371	45.804865
3501.846472	1088220.366302	45.809869
3501.612951	1087484.491227	45.814874
3501.997804	1086694.270912	45.819879
3501.413704	1085826.173582	45.824884
3501.246363	1084891.245405	45.829889
3501.186422	1083896.310431	45.834893
3501.089818	1082812.014741	45.839898
3501.022892	1081671.961655	45.844903
3500.726388	1080443.059779	45.849908
3500.578445	1079145.435137	45.854913
3499.921087	1077760.333811	45.859917
3499.389470	1076317.540859	45.864922
3499.242520	1074788.156460	45.869927
3498.663372	1073178.295175	45.874932
3498.605042	1071508.774701	45.879937
3498.544173	1069746.943788	45.884941
3498.623925	1067906.825986	45.889946
3498.144807	1065973.740692	45.894951
3497.876305	1063969.500199	45.899956
3497.676883	1061865.844944	45.904961
3497.113199	1059697.884355	45.909965
3496.858405	1057447.898172	45.914970
3496.649173	1055100.119956	45.919975
3495.767021	1052692.247527	45.924980
3495.681823	1050192.898313	45.929985
3495.441838	1047618.031926	45.934989
3494.752476	1044941.714900	45.939994
3494.480407	1042195.733984	45.944999
3493.635859	1039382.760989	45.950004
3493.365623	1036469.239825	45.955009
3493.099625	1033483.266822	45.960013
3492.368100	1030414.156301	45.965018
3491.997509	1027247.592038	45.970023
3491.292460	1024037.416891	45.975028
3491.164062	1020715.910212	45.980033
3490.145777	1017325.720853	45.985037
3489.460591	1013855.069150	45.990042
3489.018548	1010296.344166	45.995047
3488.226918	1006663.676426	46.000052
3487.670383	1002937.471521	46.005057
3486.823348	999150.834522	46.010061
3486.198622	995256.024407	46.015066
3485.619789	991301.890866	46.020071
3484.552225	987275.429739	46.025076
3483.842527	983152.533785	46.030081
3483.199128	978961.968813	46.035085
3482.994059	974693.950944	46.040090
3482.084552	970321.791437	46.045095
3481.086575	965880.411772	46.050100
3480.571659	961345.458735	46.055105
3479.432439	956748.190882	46.060109
3478.795130	952117.707035	46.065114
3478.085620	947470.849339	46.070119
3477.107443	942749.593115	46.075124
3476.020412	937936.099858	46.080129
3475.110096	933034.145150	46.085133
3474.301822	928065.646776	46.090138
3473.505028	923022.016508	46.095143
3471.690569	917898.352097	46.100148
3471.221000	912675.970160	46.105153
3470.249758	907388.425069	46.110157
3469.246337	902031.453875	46.115162
3468.202551	896582.492597	46.120167
3466.619072	891050.900802	46.125172
3465.830618	885442.577413	46.130177
3464.757347	879764.232296	46.135181
3463.364785	873996.231113	46.140186
3462.262135	868147.703384	46.145191
3460.929345	862237.239098	46.150196
3459.729721	856243.845720	46.155201
3458.371860	850160.002187	46.160205
3457.076625	844000.113104	46.165210
3455.897375	837767.640513	46.170215
3454.593653	831447.841107	46.175220
3453.301885	825050.352480	46.180225
3452.052487	818593.142369	46.185229
3450.638653	812039.270990	46.190234
3449.606661	805407.342493	46.195239
3447.960674	798687.819834	46.200244
3446.644391	791889.189382	46.205249
3445.114587	785026.515137	46.210253
3443.598013	778082.647829	46.215258
3442.152209	771046.859539	46.220263
3440.275839	763949.910412	46.225268
3439.172025	756785.273254	46.230273
3437.621624	749528.564691	46.235277
3436.170278	742183.810635	46.240282
3434.308208	734770.480108	46.245287
3432.286411	727279.400010	46.250292
3431.087145	719712.060603	46.255297
3429.273423	712085.056457	46.260301
3427.938327	704365.187826	46.265306
3426.464111	696568.361566	46.270311
3424.313723	688707.546246	46.275316
3422.644196	680771.368319	46.280321
3420.855601	672756.338986	46.285325
3418.755807	664658.396505	46.290330
3417.204289	656505.014543	46.295335
3415.523797	648278.677798	46.300340
3413.545747	639968.087910	46.305345
3411.584160	631590.526113	46.310349
3409.403341	623156.711092	46.315354
3407.755915	614644.190209	46.320359
3405.658798	606061.246344	46.325364
3403.862935	597402.297283	46.330369
3401.765486	588693.436632	46.335373
3399.599609	579914.731259	46.340378
3397.493714	571050.844390	46.345383
3395.270813	562126.444262	46.350388
3393.026698	553142.641415	46.355393
3390.541154	544106.406862	46.360397
3388.624826	534993.479150	46.365402
3386.409677	525811.630984	46.370407
3383.856266	516588.381354	46.375412
3382.139588	507279.837450	46.380417
3379.505546	497930.206865	46.385421
3377.013271	488510.255907	46.390426
3374.708136	479026.915269	46.395431
3371.978700	469485.219137	46.400436
3369.540524	459904.445818	46.405441
3367.223188	450256.646932	46.410445
3364.307659	440552.121866	46.415450
3361.844879	430800.649724	46.420455
3358.957743	420987.520647	46.425460
3356.201406	411117.454904	46.430465
3353.434663	401210.317223	46.435469
3351.226451	391265.429853	46.440474
3348.254160	381242.796413	46.445479
3345.330444	371205.959923	46.450484
3342.372384	361115.542432	46.455489
3338.943698	350979.130075	46.460493
3335.830952	340792.593190	46.465498
3332.870374	330592.075833	46.470503
3329.236472	320342.098180	46.475508
3326.717071	310055.896268	46.480513
3323.434102	299755.955559	46.485517
3319.961575	289399.432971	46.490522
3316.424625	279029.197122	46.495527
3312.992658	268632.399753	46.500532
3309.778966	258187.620680	46.505537
3306.142110	247736.857307	46.510541
3302.265687	237260.800304	46.515546
3298.680201	226700.186565	46.520551
3294.482928	216174.838226	46.525556
3290.768329	205641.671355	46.530561
3286.673187	195111.197645	46.535565
3282.622253	184584.395833	46.540570
3278.215250	174042.545341	46.545575
3273.706686	163510.107261	46.550580
3269.332017	152989.333370	46.555585
3264.810451	142468.331762	46.560589
3259.815534	131960.204215	46.565594
3255.101993	121463.920888	46.570599
3249.334425	111008.640080	46.575604
3244.222041	100577.271896	46.580609
3238.366974	90196.721173	46.585613
3232.286412	79845.831144	46.590618
3225.901773	69545.075489	46.595623
3218.809784	59344.441862	46.600628
3211.165988	49201.512215	46.605633
3202.473922	39191.270769	46.610637
3187.496804	29454.163505	46.615642
3156.272050	20344.358634	46.620647
3109.879743	12008.683883	46.625652
3048.688948	4715.131717	46.630657
2909.911075	515.739160	46.635661
2686.035233	418.379937	46.640666
2573.612350	389.696221	46.645671
2571.615791	379.826244	46.650676
2639.051958	361.194941	46.655681
2728.305347	365.392675	46.660685
2802.405248	364.961646	46.665690
2846.969477	356.530246	46.670695
2862.870279	348.995860	46.675700
2859.225639	344.835168	46.680705
2846.204085	342.002375	46.685709
2832.232336	354.553128	46.690714
2822.294931	358.532402	46.695719
2816.625093	350.288455	46.700724
2814.309191	334.649222	46.705729
2813.404154	335.772028	46.710733
2811.913320	334.944046	46.715738
2810.232814	336.648329	46.720743
2808.229522	335.346918	46.725748
2805.720816	327.939883	46.730753
2803.431320	330.143835	46.735757
2799.838293	320.450389	46.740762
2796.919165	327.039823	46.745767
2793.282822	328.109268	46.750772
2790.297837	339.630949	46.755777
2787.452598	330.782554	46.760781
2784.667053	329.961043	46.765786
2781.637838	312.566908	46.770791
2778.102423	313.954270	46.775796
2775.250290	320.535525	46.780801
2771.970419	319.098100	46.785805
2768.468772	318.951977	46.790810
2765.323982	302.509831	46.795815
2761.878602	307.085989	46.800820
2758.757754	309.736011	46.805825
2755.290656	306.643194	46.810829
2751.873542	312.337231	46.815834
2748.952115	304.026886	46.820839
2745.765854	305.281717	46.825844
2742.688170	309.330410	46.830849
2738.923200	315.268860	46.835853
2735.455969	321.685752	46.840858
2732.190139	305.684751	46.845863
2728.908971	305.376901	46.850868
2725.722432	299.927169	46.855873
2722.261822	296.833596	46.860877
2718.758586	300.629845	46.865882
2715.588760	287.806612	46.870887
2711.648659	301.799390	46.875892
2708.111657	296.340361	46.880897
2705.337188	292.814414	46.885901
2702.121904	292.067340	46.890906
2698.526194	298.075763	46.895911
2695.177220	294.087910	46.900916
2691.723217	297.726191	46.905921
2688.396574	289.785078	46.910925
2684.322104	286.503372	46.915930
2681.275166	280.027594	46.920935
2678.365004	294.094054	46.925940
2674.999495	290.049842	46.930945
2671.227830	287.692368	46.935949
2667.790566	292.749165	46.940954
2665.072629	287.055965	46.945959
2660.802292	288.048174	46.950964
2656.938878	288.324319	46.955969
2653.909612	279.264153	46.960973
2650.634558	293.304455	46.965978
2647.269036	284.176507	46.970983
2643.983539	283.541568	46.975988
2640.175623	280.079297	46.980993
2636.458960	279.801364	46.985997
2632.778402	276.850753	46.991002
2630.313347	277.364380	46.996007
2626.994639	279.788192	47.001012
2623.410249	284.571119	47.006017
2619.232107	283.892766	47.011021
2615.653192	277.355859	47.016026
2612.787503	274.542111	47.021031
2609.723922	279.434313	47.026036
2605.552344	285.975368	47.031041
2601.867734	276.925122	47.036045
2597.785589	284.008752	47.041050
2595.729323	276.780086	47.046055
2592.080066	272.690855	47.051060
2588.579188	279.276613	47.056065
2584.863183	277.087987	47.061069
2581.606649	273.450677	47.066074
2578.618746	272.958191	47.071079
2574.451099	263.865083	47.076084
2570.815375	270.058026	47.081089
2567.768816	268.995700	47.086093
2564.301180	273.899787	47.091098
2560.652509	267.563642	47.096103
2557.060249	277.233528	47.101108
2553.549400	270.621899	47.106113
2550.499820	266.525363	47.111117
2546.244821	266.399778	47.116122
2543.439627	257.762477	47.121127
2539.960533	264.154936	47.126132
2536.422074	262.067190	47.131137
2533.000183	256.906865	47.136141
2529.627653	267.543182	47.141146
2525.948512	258.918192	47.146151
2522.853599	259.067484	47.151156
2518.752256	263.094634	47.156161
2515.363913	253.315057	47.161165
2512.038113	262.293324	47.166170
2508.307122	262.857098	47.171175
2504.627824	261.905846	47.176180
2501.882345	267.090634	47.181185
2498.121811	258.316395	47.186189
2494.604713	262.984780	47.191194
2491.023566	254.862692	47.196199
2487.484768	260.586349	47.201204
2484.227664	260.740697	47.206209
2481.142596	252.515304	47.211213
2477.201583	256.061321	47.216218
2473.846950	258.261639	47.221223
2470.029098	261.870619	47.226228
2466.725226	256.252727	47.231233
2463.198303	255.447342	47.236237
2459.710769	261.609378	47.241242
2456.381356	250.543783	47.246247
2452.810114	254.283963	47.251252
2449.334041	258.282227	47.256257
2446.113589	251.390534	47.261261
2442.384748	259.004456	47.266266
2439.094031	250.556389	47.271271
2435.203105	251.099019	47.276276
2431.554032	251.638469	47.281281
2428.522784	259.283469	47.286285
2424.683542	255.430869	47.291290
2421.697387	255.699598	47.296295
2418.104187	251.312843	47.301300
2414.356329	247.002208	47.306305
2411.133712	244.211991	47.311309
2407.521283	250.383195	47.316314
2403.962875	250.007752	47.321319
2400.566240	254.685215	47.326324
2396.962542	249.392454	47.331329
2393.551553	240.355140	47.336333
2389.982232	243.381142	47.341338
2386.801162	238.227256	47.346343
2383.552407	253.551036	47.351348
2379.526114	247.023725	47.356353
2375.926603	236.805603	47.361357
2372.562597	250.734431	47.366362
2368.755834	230.826813	47.371367
2365.305624	241.236930	47.376372
2362.015700	239.370220	47.381377
2358.525191	232.280717	47.386381
2354.987342	242.738539	47.391386
2351.853285	237.158017	47.396391
2348.105216	243.093722	47.401396
2344.757782	244.085042	47.406401
2341.070281	242.144112	47.411405
2337.728990	239.199963	47.416410
2334.169492	233.879530	47.421415
2330.430403	245.046453	47.426420
2326.941498	231.875556	47.431425
2323.843216	232.816816	47.436429
2320.079678	238.977260	47.441434
2316.751416	223.982936	47.446439
2313.460405	225.207364	47.451444
2309.606761	234.488009	47.456449
2306.175766	229.160705	47.461453
2302.398657	238.762195	47.466458
2299.099506	229.941101	47.471463
2295.715240	238.653521	47.476468
2292.108374	238.520337	47.481473
2288.699942	231.963896	47.486477
2285.062746	236.121688	47.491482
2281.614455	239.620373	47.496487
2278.398679	238.155242	47.501492
2274.900671	243.641197	47.506497
2271.397249	241.555993	47.511501
2267.624815	232.576096	47.516506
2264.165125	238.200859	47.521511
2260.576929	234.258706	47.526516
2256.912695	226.602516	47.531521
2253.622480	229.581359	47.536525
2250.341484	241.510554	47.541530
2246.930267	235.867666	47.546535
2243.539901	223.583092	47.551540
2239.564827	234.338594	47.556545
2236.271533	226.410898	47.561549
2232.861431	225.942608	47.566554
2230.028323	241.547504	47.571559
2226.290904	235.015069	47.576564
2222.296842	234.774018	47.581569
2218.699477	231.040087	47.586573
2215.003350	234.411663	47.591578
2211.864030	228.275356	47.596583
2208.218663	228.929632	47.601588
2204.563315	221.177890	47.606593
2201.400868	226.385656	47.611597
2197.814155	232.779118	47.616602
2194.307271	222.898929	47.621607
2190.877507	227.313487	47.626612
2187.167066	226.898111	47.631617
2184.194117	218.680437	47.636621
2180.097030	237.171178	47.641626
2176.746717	226.409913	47.646631
2173.277369	221.683021	47.651636
2170.079902	221.914093	47.656641
2166.739999	218.878246	47.661645
2162.706193	227.526676	47.666650
2159.132919	216.375018	47.671655
2156.115697	222.096921	47.676660
2152.125986	229.019377	47.681665
2148.733042	221.298970	47.686669
2145.218547	237.049420	47.691674
2141.637685	222.689108	47.696679
2138.093555	225.361818	47.701684
2134.749433	225.781162	47.706689
2131.581155	214.985760	47.711693
2127.778344	226.194631	47.716698
2124.700155	224.965357	47.721703
2120.907737	217.969692	47.726708
2117.028008	226.707958	47.731713
2113.766601	226.564837	47.736717
2110.469313	215.743963	47.741722
2106.940917	219.419209	47.746727
2103.428986	221.548547	47.751732
2099.887769	218.963556	47.756737
2096.770813	221.063558	47.761741
2092.821559	226.364153	47.766746
2089.256395	222.062340	47.771751
2085.759147	221.983588	47.776756
2081.988417	213.053652	47.781761
2078.770059	216.845780	47.786765
2075.421891	216.711168	47.791770
2071.619409	211.677411	47.796775
2068.487265	216.634766	47.801780
2064.733872	213.674281	47.806785
2061.450805	220.514543	47.811789
2057.769661	210.051810	47.816794
2054.317045	215.754606	47.821799
2050.786269	218.011483	47.826804
2047.156100	209.731914	47.831809
2044.188777	214.929153	47.836813
2040.414251	212.781747	47.841818
2036.981385	213.188939	47.846823
2033.614374	220.257933	47.851828
2029.818996	218.369987	47.856833
2026.325517	205.090838	47.861837
2022.642561	212.457213	47.866842
2019.759675	211.367234	47.871847
2015.726177	208.903945	47.876852
2012.191968	219.006111	47.881857
2008.865364	203.091549	47.886861
2005.493544	215.831057	47.891866
2002.132578	210.680800	47.896871
1998.530733	205.842577	47.901876
1994.271071	212.288625	47.906881
1991.100940	203.556530	47.911885
1987.632451	208.134420	47.916890
1984.402455	209.873581	47.921895
1981.130840	202.272366	47.926900
1977.659079	213.829293	47.931905
1974.382841	202.296480	47.936909
1970.201685	221.964607	47.941914
1966.684600	207.712289	47.946919
1963.326073	206.519469	47.951924
1959.691089	219.240748	47.956929
1956.351148	198.607396	47.961933
1952.868422	212.926359	47.966938
1949.615763	210.106197	47.971943
1945.991252	204.494326	47.976948
1942.429928	213.388200	47.981953
1938.682356	203.803697	47.986957
1935.250448	206.694562	47.991962
1931.597092	206.293774	47.996967
1928.365232	204.289932	48.001972
1924.640528	207.408562	48.006977
1921.575240	197.497922	48.011981
1918.116100	208.748823	48.016986
1914.624522	208.630347	48.021991
1911.097374	200.960535	48.026996
1906.980800	210.880798	48.032001
1903.795231	193.334643	48.037005
1900.315293	206.375455	48.042010
1896.777462	211.266221	48.047015
1893.496130	199.438425	48.052020
1889.462341	201.370810	48.057025
1886.479918	210.993968	48.062029
1883.263363	197.154634	48.067034
1879.384318	203.158806	48.072039
1875.520443	207.190107	48.077044
1871.704393	209.843769	48.082049
1868.822575	203.255536	48.087053
1865.318298	219.745183	48.092058
1862.208495	197.773236	48.097063
1858.746188	205.339063	48.102068
1855.273551	205.790786	48.107073
1851.688002	200.359200	48.112077
1847.911728	204.005407	48.117082
1843.952620	202.185815	48.122087
1840.743125	206.484458	48.127092
1837.313146	200.093230	48.132097
1833.762167	199.623906	48.137101
1830.083986	213.738776	48.142106
1826.748423	197.239497	48.147111
1823.089718	201.423530	48.152116
1819.393154	212.935521	48.157121
1816.139548	189.357041	48.162125
1813.077289	198.750000	48.167130
1809.693809	199.240801	48.172135
1806.411751	189.265659	48.177140
1802.062581	191.837625	48.182145
1798.836804	192.952559	48.187149
1794.698117	198.239459	48.192154
1791.845733	207.615955	48.197159
1788.508144	202.142012	48.202164
1784.876369	203.520365	48.207169
1781.043961	197.271336	48.212173
1777.489399	199.694057	48.217178
1773.969258	196.816302	48.222183
1770.586381	195.613385	48.227188
1767.166835	198.218251	48.232193
1764.203569	192.906019	48.237197
1760.792160	205.376682	48.242202
1756.923589	191.341345	48.247207
1753.205754	193.463083	48.252212
1749.244592	198.432441	48.257217
1745.900893	187.105749	48.262221
1742.661039	199.927934	48.267226
1739.605335	195.321758	48.272231
1736.315934	189.245392	48.277236
1732.589712	200.869640	48.282241
1729.240094	187.042497	48.287245
1725.048847	197.805746	48.292250
1721.529656	198.421091	48.297255
1718.390328	191.061509	48.302260
1714.372661	196.682757	48.307265
1711.385786	185.251235	48.312269
1707.372676	198.761587	48.317274
1704.123437	184.929343	48.322279
1700.954315	193.396419	48.327284
1696.927234	194.731619	48.332289
1693.845121	188.453652	48.337293
1690.273758	189.708035	48.342298
1686.877970	183.379723	48.347303
1683.584386	187.066719	48.352308
1679.620760	190.151094	48.357313
1676.433910	186.432203	48.362317
1672.825886	191.185969	48.367322
1668.911250	189.879750	48.372327
1665.211190	188.935317	48.377332
1662.305866	193.050947	48.382337
1659.112295	182.910150	48.387341
1655.212534	184.034943	48.392346
1651.686288	185.214222	48.397351
1648.501765	181.265191	48.402356
1644.686627	195.250781	48.407361
1641.328909	181.941501	48.412365
1637.868609	184.078216	48.417370
1634.165924	183.238908	48.422375
1630.655801	171.011403	48.427380
1627.183520	185.917605	48.432385
1623.916906	188.559451	48.437389
1620.456139	185.749327	48.442394
1616.576107	190.010327	48.447399
1613.278211	187.665428	48.452404
1609.534680	191.757304	48.457409
1606.193990	184.757071	48.462413
1602.351311	179.799093	48.467418
1599.267563	184.962616	48.472423
1595.639499	179.430661	48.477428
1591.835777	184.099454	48.482433
1588.654196	186.108708	48.487437
1585.288112	174.291054	48.492442
1581.612902	178.755833	48.497447
1578.435967	181.537789	48.502452
1574.341619	187.288469	48.507457
1570.957632	183.413433	48.512461
1567.554749	180.171240	48.517466
1563.914192	181.092991	48.522471
1560.832840	179.534881	48.527476
1557.188844	187.704885	48.532481
1553.527914	194.238318	48.537485
1549.909883	183.715486	48.542490
1546.373223	179.974181	48.547495
1543.441720	187.122524	48.552500
1539.684126	190.169025	48.557505
1536.405679	176.048308	48.562509
1532.539467	179.738413	48.567514
1529.128986	179.376480	48.572519
1525.668953	180.839677	48.577524
1521.842331	180.112633	48.582529
1518.630813	178.462766	48.587533
1515.273280	185.993575	48.592538
1511.796627	177.552961	48.597543
1508.622947	184.060949	48.602548
1504.376613	180.160450	48.607553
1500.890766	175.040056	48.612557
1497.608142	185.987895	48.617562
1493.723990	175.390045	48.622567
1490.532277	169.380073	48.627572
1487.141241	191.387108	48.632577
1483.815799	178.649445	48.637581
1480.092609	183.278167	48.642586
1476.863124	185.033048	48.647591
1473.102849	187.732952	48.652596
1469.379096	185.644965	48.657601
1466.121242	181.409593	48.662605
1462.448865	181.109660	48.667610
1458.921818	183.843196	48.672615
1455.638557	174.329483	48.677620
1452.300118	177.363674	48.682625
1448.846418	177.450596	48.687629
1445.193621	177.437490	48.692634
1441.052571	181.438289	48.697639
1438.234599	177.195742	48.702644
1434.406912	176.598654	48.707649
1431.148654	182.472164	48.712653
1427.678017	176.588365	48.717658
1423.807117	183.365953	48.722663
1420.657321	184.623798	48.727668
1416.906818	193.705959	48.732673
1413.635078	182.962981	48.737677
1409.784903	180.432802	48.742682
1406.246095	186.134202	48.747687
1403.216783	182.736221	48.752692
1399.932519	177.159969	48.757697
1396.609125	181.476796	48.762701
1392.711250	173.554069	48.767706
1388.901904	175.596975	48.772711
1385.420764	176.377372	48.777716
1381.715027	176.999503	48.782721
1378.258884	175.251369	48.787725
1375.076172	178.144267	48.792730
1371.298111	180.247427	48.797735
1368.120544	170.091236	48.802740
1364.000008	183.831661	48.807745
1360.924509	174.091429	48.812749
1357.406533	171.631942	48.817754
1353.998609	188.617050	48.822759
1350.775154	178.955996	48.827764
1347.061124	190.076416	48.832769
1343.656123	175.210841	48.837773
1339.908869	174.531964	48.842778
1336.190603	181.452510	48.847783
1332.541379	176.406432	48.852788
1329.526745	169.841084	48.857793
1326.133554	175.528249	48.862797
1322.635991	176.881916	48.867802
1318.971027	184.217794	48.872807
1315.677341	173.003475	48.877812
1311.973576	186.256437	48.882817
1308.491035	181.013663	48.887821
1304.826387	173.886830	48.892826
1301.171776	182.353873	48.897831
1297.949883	176.994486	48.902836
1294.309031	182.144718	48.907841
1291.031371	169.884878	48.912845
1287.395880	178.963790	48.917850
1283.903235	174.446242	48.922855
1280.479188	171.202072	48.927860
1276.760115	176.848340	48.932865
1273.320317	171.338477	48.937869
1269.908665	174.261218	48.942874
1266.164886	164.116570	48.947879
1263.040658	167.923673	48.952884
1259.262229	173.128494	48.957889
1256.047619	166.205617	48.962893
1252.518284	169.802866	48.967898
1248.741293	173.082383	48.972903
1245.713810	170.314392	48.977908
1241.842337	186.194449	48.982913
1238.388170	168.922855	48.987917
1235.150635	172.420348	48.992922
1231.375522	173.084988	48.997927
1227.987552	164.680718	49.002932
1224.131889	166.281386	49.007937
1220.869223	172.979284	49.012941
1217.278428	167.524864	49.017946
1213.673540	171.777938	49.022951
1210.444213	157.876932	49.027956
1206.810120	171.084089	49.032961
1203.543925	169.436199	49.037965
1199.944493	168.898838	49.042970
1196.471905	172.873575	49.047975
1192.947049	171.938854	49.052980
1188.946922	165.827889	49.057985
1185.773136	176.237457	49.062989
1182.394242	171.164896	49.067994
1178.569978	174.890779	49.072999
1175.839787	155.647468	49.078004
1172.142215	167.893456	49.083009
1168.357634	165.510837	49.088013
1165.125311	169.542311	49.093018
1161.484714	171.132470	49.098023
1157.653403	158.763946	49.103028
1154.122805	167.928195	49.108033
1150.718892	173.256322	49.113037
1147.015709	169.114070	49.118042
1143.151246	168.494015	49.123047
1140.569589	165.570196	49.128052
1136.484430	163.719741	49.133057
1133.230147	163.428014	49.138061
1129.934897	158.260485	49.143066
1125.931560	158.905244	49.148071
1123.073814	160.652975	49.153076
1119.280924	163.097497	49.158081
1116.421129	164.572096	49.163085
1112.451439	160.559005	49.168090
1108.534794	176.164702	49.173095
1105.460957	159.432026	49.178100
1101.105973	162.662706	49.183105
1098.223642	167.986037	49.188109
1094.876370	160.632520	49.193114
1091.064735	156.903719	49.198119
1087.751792	158.643546	49.203124
1083.782040	164.459836	49.208129
1080.623438	156.934202	49.213133
1077.443631	159.579514	49.218138
1073.684946	165.082361	49.223143
1070.741508	152.724280	49.228148
1067.035428	168.836350	49.233153
1063.052587	158.418568	49.238157
1059.668511	169.617412	49.243162
1056.040321	157.672595	49.248167
1053.161635	156.803322	49.253172
1049.278210	166.432228	49.258177
1045.653195	160.290702	49.263181
1042.617306	155.916408	49.268186
1038.535655	162.439318	49.273191
1034.923819	159.345462	49.278196
1031.414497	161.734039	49.283201
1028.064906	154.648598	49.288205
1024.660489	159.309159	49.293210
1020.695565	162.346643	49.298215
1017.749497	151.603427	49.303220
1014.404395	164.806251	49.308225
1011.159363	165.287008	49.313229
1007.698790	148.646078	49.318234
1003.532145	174.505315	49.323239
999.997187	154.592223	49.328244
996.177015	161.886878	49.333249
992.838605	159.129205	49.338253
990.055458	159.712180	49.343258
985.895826	162.301774	49.348263
982.696552	152.695064	49.353268
979.111405	165.797246	49.358273
975.788445	162.870993	49.363277
972.202054	149.041332	49.368282
968.794082	159.741006	49.373287
965.176461	151.797949	49.378292
962.205230	162.246654	49.383297
958.678350	169.292141	49.388301
954.881540	152.984672	49.393306
950.628653	150.835874	49.398311
947.232388	156.321658	49.403316
943.791427	149.800075	49.408321
940.484164	157.292123	49.413325
937.192205	150.772775	49.418330
933.596790	158.874345	49.423335
930.133283	154.037679	49.428340
926.301649	162.403981	49.433345
922.843937	161.380576	49.438349
919.610932	151.074876	49.443354
916.150522	156.106303	49.448359
912.758993	159.031312	49.453364
909.313734	161.964209	49.458369
905.433574	158.696901	49.463373
902.001594	147.915895	49.468378
898.145755	161.165108	49.473383
895.026564	155.424749	49.478388
891.994190	164.251125	49.483393
888.075187	159.897336	49.488397
884.868666	156.716613	49.493402
881.062181	162.933228	49.498407
877.868121	151.913072	49.503412
873.965310	149.295817	49.508417
870.227426	152.211247	49.513421
866.679765	154.538558	49.518426
863.233488	159.407657	49.523431
859.909742	145.535890	49.528436
856.608729	152.193991	49.533441
853.203807	149.900402	49.538445
849.839720	149.310261	49.543450
845.877804	156.354822	49.548455
842.801735	146.291500	49.553460
839.118875	149.908376	49.558465
835.636821	159.827049	49.563469
832.039935	160.823359	49.568474
828.311580	151.928299	49.573479
825.099406	153.012027	49.578484
821.614455	157.775360	49.583489
817.826999	153.609439	49.588493
814.451871	161.689881	49.593498
810.774271	155.180813	49.598503
807.390384	158.422676	49.603508
803.661841	159.437979	49.608513
800.400380	153.784995	49.613517
797.354173	154.299120	49.618522
793.502614	152.946004	49.623527
789.952562	150.467956	49.628532
786.607668	145.994766	49.633537
782.944195	145.948362	49.638541
779.410544	154.120105	49.643546
775.825073	152.407658	49.648551
772.867772	143.502215	49.653556
769.007864	153.283533	49.658561
765.270866	157.256655	49.663565
761.560527	148.101471	49.668570
758.201179	152.854548	49.673575
755.152908	144.912214	49.678580
751.662509	153.438792	49.683585
748.149157	152.361233	49.688589
744.166078	152.448824	49.693594
740.898440	155.416890	49.698599
737.445404	151.281129	49.703604
734.057347	153.820796	49.708609
729.991306	146.162868	49.713613
726.995712	146.184764	49.718618
723.047565	153.646989	49.723623
719.838103	155.293049	49.728628
716.522061	168.697471	49.733633
712.837040	151.002092	49.738637
709.622158	152.793482	49.743642
705.898569	157.467042	49.748647
702.284680	150.988070	49.753652
699.122558	145.864992	49.758657
695.313251	147.171605	49.763661
692.050298	146.984324	49.768666
688.527512	147.877414	49.773671
685.022702	136.732212	49.778676
681.521160	149.158814	49.783681
677.909881	150.081914	49.788685
674.316138	145.578755	49.793690
670.571710	151.174548	49.798695
667.353811	149.880327	49.803700
663.858114	153.983238	49.808705
660.071851	154.440985	49.813709
656.917767	144.392530	49.818714
653.110710	144.801133	49.823719
650.241025	143.034962	49.828724
646.184564	139.538263	49.833729
642.529611	150.758709	49.838733
639.455304	148.555457	49.843738
635.785837	147.792409	49.848743
632.892518	145.512308	49.853748
629.206738	147.365330	49.858753
625.511702	147.792442	49.863757
622.037067	148.529533	49.868762
618.024385	155.920096	49.873767
614.466804	145.990891	49.878772
610.892551	146.827804	49.883777
607.455136	143.603577	49.888781
604.517935	140.643311	49.893786
600.990367	163.161234	49.898791
597.484062	140.250929	49.903796
593.724305	148.133746	49.908801
590.036136	147.955877	49.913805
586.680480	139.731644	49.918810
582.999151	160.543472	49.923815
579.747504	152.654551	49.928820
576.486405	144.738292	49.933825
572.741324	143.901643	49.938829
569.711691	144.378704	49.943834
565.665445	146.845739	49.948839
562.229464	146.326024	49.953844
558.692273	148.777548	49.958849
554.842444	151.777834	49.963853
551.965695	132.197377	49.968858
548.190722	148.575435	49.973863
544.909916	148.473553	49.978868
541.095476	149.485629	49.983873
537.532855	153.259394	49.988877
534.630768	143.952216	49.993882
530.793209	144.082787	49.998887
527.419754	136.003496	50.003892
523.920769	144.190932	50.008897
520.315578	144.828197	50.013901
516.821285	143.235007	50.018906
512.966331	152.352668	50.023911
509.694951	137.530531	50.028916
505.884572	142.698877	50.033921
502.730424	135.689889	50.038925
499.542669	134.139798	50.043930
495.730014	143.895975	50.048935
492.126442	140.559466	50.053940
488.278997	149.551297	50.058945
484.983246	149.907798	50.063949
482.010636	136.854637	50.068954
477.794858	147.354974	50.073959
474.467491	135.144725	50.078964
471.051792	139.812333	50.083969
467.860782	151.131135	50.088973
464.350531	136.669213	50.093978
460.779552	147.306430	50.098983
457.054121	146.440360	50.103988
453.376709	139.958821	50.108993
449.968674	142.460096	50.113997
446.747023	146.438129	50.119002
443.227274	143.007595	50.124007
439.680442	131.503688	50.129012
436.161529	144.178214	50.134017
432.258356	143.614005	50.139021
429.161312	137.714666	50.144026
425.138243	147.041171	50.149031
422.120902	135.991518	50.154036
418.564682	142.090661	50.159041
415.073746	144.921541	50.164045
412.105991	138.512906	50.169050
408.278603	145.281927	50.174055
404.866008	144.011420	50.179060
400.950161	138.873717	50.184065
397.241528	155.532901	50.189069
393.906155	142.410378	50.194074
391.053449	142.221576	50.199079
386.983671	144.644066	50.204084
383.423867	141.239028	50.209089
379.851095	144.771167	50.214093
376.669670	145.062567	50.219098
372.919724	142.089287	50.224103
369.526072	146.186532	50.229108
366.284396	139.181029	50.234113
362.628685	136.549418	50.239117
359.169578	135.166064	50.244122
355.371660	153.055537	50.249127
352.245064	140.015656	50.254132
348.553249	138.699560	50.259137
344.640913	148.758674	50.264141
341.516237	132.946686	50.269146
338.032516	144.501628	50.274151
334.716149	139.083407	50.279156
331.222329	133.302354	50.284161
327.517405	139.711121	50.289165
324.203216	142.514524	50.294170
320.409299	147.491426	50.299175
316.825293	145.184209	50.304180
313.553555	141.489621	50.309185
309.674210	139.767192	50.314189
306.541231	143.903778	50.319194
302.615984	141.966076	50.324199
299.682709	146.311574	50.329204
296.344205	145.276804	50.334209
292.426091	137.045936	50.339213
288.836639	125.932054	50.344218
285.423894	140.634602	50.349223
282.285684	141.670954	50.354228
278.605425	132.799303	50.359233
274.868692	142.825294	50.364237
271.435410	139.411455	50.369242
268.010145	137.247727	50.374247
264.468488	145.456834	50.379252
261.088557	127.986961	50.384257
257.251028	134.521553	50.389261
253.907540	132.674027	50.394266
250.239219	146.190077	50.399271
247.199683	136.891465	50.404276
243.737914	138.083400	50.409281
239.812033	143.275313	50.414285
236.431974	136.983333	50.419290
232.603892	150.372776	50.424295
229.700340	146.393554	50.429300
225.753989	138.253523	50.434305
222.038267	141.234107	50.439309
218.992286	135.733495	50.444314
215.436759	143.587194	50.449319
212.138782	138.219279	50.454324
208.287393	138.105691	50.459329
204.891042	141.428233	50.464333
201.683222	136.169635	50.469338
198.169657	138.780517	50.474343
194.569083	132.772129	50.479348
190.875677	134.500767	50.484353
187.220563	138.842259	50.489357
184.056238	139.738542	50.494362
180.260974	137.500841	50.499367
176.802438	134.395679	50.504372
173.503105	134.127560	50.509377
169.675650	139.080190	50.514381
166.044940	138.822927	50.519386
162.513335	145.542415	50.524391
159.194097	128.953338	50.529396
156.146303	131.570644	50.534401
152.590490	132.224222	50.539405
149.277193	135.254172	50.544410
145.331763	147.088024	50.549415
141.957217	135.902026	50.554420
138.427859	136.767689	50.559425
134.513604	147.194417	50.564429
131.302609	131.936966	50.569434
127.757041	145.372704	50.574439
124.381055	137.696390	50.579444
121.171455	133.416488	50.584449
117.341616	140.870430	50.589453
113.488320	137.911331	50.594458
109.986795	132.537156	50.599463
107.026081	133.668666	50.604468
103.604343	135.930577	50.609473
99.738883	130.270763	50.614477
96.247695	129.821492	50.619482
92.940148	134.908448	50.624487
89.165442	135.621021	50.629492
85.900331	130.057053	50.634497
82.146014	134.669421	50.639501
78.910721	129.723532	50.644506
75.263284	132.289219	50.649511
71.733195	131.546578	50.654516
68.691788	130.205745	50.659521
64.649395	135.950727	50.664525
60.803439	136.787162	50.669530
57.601216	127.937889	50.674535
54.374967	120.553071	50.679540
50.931247	127.485678	50.684545
46.880090	135.310469	50.689549
43.922602	130.171203	50.694554
40.395254	139.534078	50.699559
37.023750	121.925754	50.704564
33.315962	123.562445	50.709569
29.509403	134.389025	50.714573
25.807284	131.842336	50.719578
22.623778	146.009395	50.724583
19.003057	134.546000	50.729588
15.925538	132.890731	50.734593
12.389661	137.661290	50.739597
8.992472	131.666073	50.744602
5.218805	137.134153	50.749607
1.416836	130.442249	50.754612