Thu Jun 16 11:07:25 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.641635	109.702263	0.000000
0.491628	111.184808	0.005005
0.940101	110.597145	0.010010
0.876198	112.759098	0.015014
0.312975	103.331802	0.020019
0.485503	87.273244	0.025024
0.306159	89.226084	0.030029
0.391835	74.581298	0.035034
-0.039595	64.579489	0.040038
-0.420035	56.805740	0.045043
-0.354082	45.174365	0.050048
-1.235999	27.965794	0.055053
-1.485202	20.301191	0.060058
-1.832817	19.890864	0.065062
-1.908286	7.434863	0.070067
-2.090529	10.744756	0.075072
-2.648902	-1.538307	0.080077
-2.634463	-0.367168	0.085082
-3.332420	-5.062517	0.090086
-3.739878	0.605806	0.095091
-3.861707	4.817666	0.100096
-4.626389	8.154851	0.105101
-4.402597	1.576105	0.110106
-4.838951	5.609981	0.115110
-4.917005	-8.045403	0.120115
-4.714860	1.542502	0.125120
-5.325085	-9.407663	0.130125
-5.562765	1.300920	0.135130
-5.918222	3.509854	0.140134
-5.845116	-3.449059	0.145139
-5.863685	-4.721338	0.150144
-6.834665	-5.923139	0.155149
-7.009704	-14.319360	0.160154
-7.389573	-2.144084	0.165158
-7.994210	-4.274674	0.170163
-7.603118	-1.274891	0.175168
-7.986134	2.395906	0.180173
-7.625857	-1.968230	0.185178
-7.583475	1.000983	0.190182
-8.833148	0.368101	0.195187
-8.991739	3.994707	0.200192
-9.501843	-1.908029	0.205197
-9.280469	5.561671	0.210202
-9.086676	-6.107759	0.215206
-9.726217	2.436681	0.220211
-10.516907	-10.591289	0.225216
-10.883465	5.254360	0.230221
-10.851088	5.152175	0.235226
-11.093802	-7.045819	0.240230
-11.110805	7.220732	0.245235
-10.838612	-4.901156	0.250240
-11.042710	-0.286416	0.255245
-11.873078	1.875810	0.260250
-12.224499	0.228704	0.265254
-12.338379	-1.517047	0.270259
-12.373673	1.923742	0.275264
-12.779712	0.197071	0.280269
-13.128704	3.027638	0.285274
-13.752094	-0.562093	0.290278
-13.828368	-5.233211	0.295283
-13.757930	-3.995561	0.300288
-13.835763	-0.707956	0.305293
-14.130766	0.282484	0.310298
-14.988265	-4.079291	0.315302
-15.579453	0.799389	0.320307
-15.488820	2.299868	0.325312
-15.416664	0.292624	0.330317
-15.625522	0.294034	0.335322
-15.739632	2.739512	0.340326
-15.684776	11.911866	0.345331
-15.695294	-5.554217	0.350336
-16.681418	10.516746	0.355341
-16.817157	2.398342	0.360346
-17.396281	-6.834473	0.365350
-17.363534	2.895074	0.370355
-17.192794	-6.480998	0.375360
-18.261640	-4.342500	0.380365
-18.560428	-1.602705	0.385370
-18.907320	2.061234	0.390374
-19.239204	-6.777476	0.395379
-18.901252	-8.054906	0.400384
-19.294533	-1.904736	0.405389
-19.241020	-4.769452	0.410394
-19.234691	-6.825305	0.415398
-19.578385	-5.764568	0.420403
-20.114758	-12.915262	0.425408
-20.599892	7.042911	0.430413
-20.416260	-6.041009	0.435418
-20.310431	-2.623050	0.440422
-20.901711	-2.853809	0.445427
-21.486648	-13.330663	0.450432
-22.338760	-1.332858	0.455437
-22.076496	-5.951205	0.460442
-22.341561	-5.686670	0.465446
-22.491264	8.478099	0.470451
-22.055552	0.428137	0.475456
-22.664441	1.781898	0.480461
-22.523281	-9.476423	0.485466
-23.658080	-7.139387	0.490470
-23.674745	-12.252158	0.495475
-23.774995	-5.054179	0.500480
-23.904274	-4.723987	0.505485
-24.540337	-13.037014	0.510490
-25.083592	-6.697113	0.515494
-25.572362	-2.477297	0.520499
-25.326595	-5.134846	0.525504
-25.522949	-1.993491	0.530509
-25.535205	-3.392596	0.535514
-25.805342	-3.909939	0.540518
-25.777114	-9.243813	0.545523
-25.667941	3.813504	0.550528
-26.556046	0.020493	0.555533
-26.540907	-12.184296	0.560538
-26.921268	2.399092	0.565542
-28.193273	-6.076194	0.570547
-28.396143	-11.605684	0.575552
-28.323456	-1.152609	0.580557
-27.708898	-13.968171	0.585562
-28.245433	-6.121859	0.590566
-28.752789	-1.870559	0.595571
-28.907616	-11.594046	0.600576
-29.039203	-2.162508	0.605581
-29.277488	-11.915512	0.610586
-29.664994	-12.560353	0.615590
-30.350099	-8.416413	0.620595
-30.197019	-13.439344	0.625600
-30.594038	5.130319	0.630605
-30.418739	-12.132851	0.635610
-30.405062	-10.130532	0.640614
-31.233883	-5.213076	0.645619
-31.515816	-18.543430	0.650624
-31.824798	-5.600414	0.655629
-31.721156	-3.995639	0.660634
-31.952761	-12.351434	0.665638
-32.171202	-5.793618	0.670643
-32.670231	-8.224694	0.675648
-33.213981	0.502604	0.680653
-33.488948	-3.869510	0.685658
-33.528675	-3.460890	0.690662
-33.783161	-4.646630	0.695667
-33.866049	1.677472	0.700672
-33.958158	-9.046467	0.705677
-34.208207	-7.520665	0.710682
-35.008316	-8.661221	0.715686
-35.103182	7.177805	0.720691
-35.113228	-7.003193	0.725696
-34.868708	-10.030288	0.730701
-35.645545	-9.172422	0.735706
-36.516688	-6.607265	0.740710
-36.699002	-9.048950	0.745715
-36.741319	-6.473376	0.750720
-36.847179	-8.193124	0.755725
-36.761656	-10.479594	0.760730
-36.719574	0.928472	0.765734
-36.961233	-7.852240	0.770739
-37.593890	-11.178312	0.775744
-38.228975	10.443965	0.780749
-38.582542	-3.218962	0.785754
-38.788838	-10.413450	0.790758
-38.797914	1.437737	0.795763
-38.419861	-13.008941	0.800768
-38.929161	5.587170	0.805773
-39.539084	-1.954272	0.810778
-39.794970	5.071236	0.815782
-39.944447	5.324759	0.820787
-39.955242	-8.519902	0.825792
-40.485576	7.576261	0.830797
-40.606135	-4.964514	0.835802
-41.069547	-2.483410	0.840806
-41.805154	4.700004	0.845811
-41.629156	-8.521553	0.850816
-41.840505	-4.696421	0.855821
-41.809264	0.110965	0.860826
-41.949409	-11.054201	0.865830
-41.979835	4.366338	0.870835
-42.379797	-4.702425	0.875840
-42.943848	-3.862262	0.880845
-43.386721	-3.551472	0.885850
-43.106952	-5.801678	0.890854
-43.507437	-1.283128	0.895859
-44.018777	6.356392	0.900864
-44.899166	1.730659	0.905869
-45.074737	1.396771	0.910874
-44.923984	-1.399469	0.915878
-45.674226	2.880924	0.920883
-45.263252	-2.791349	0.925888
-45.122917	3.322627	0.930893
-44.889617	-2.072466	0.935898
-45.317786	-4.048127	0.940902
-45.874895	3.557225	0.945907
-45.890592	-1.419961	0.950912
-46.345605	-0.131582	0.955917
-47.543943	-4.405849	0.960922
-47.692082	-7.766711	0.965926
-48.228253	1.700023	0.970931
-47.627024	-11.491475	0.975936
-47.886192	-2.993226	0.980941
-48.064306	-9.702852	0.985946
-47.773708	-9.826501	0.990950
-48.471699	-5.392263	0.995955
-49.096951	-14.756348	1.000960
-49.561920	-3.325360	1.005965
-49.472920	-5.773999	1.010970
-49.506565	-13.614192	1.015974
-49.785812	-4.426689	1.020979
-49.883710	-14.518974	1.025984
-50.704929	-0.831214	1.030989
-50.801629	-2.985070	1.035994
-50.943937	-4.306055	1.040998
-51.170380	-2.854493	1.046003
-51.196568	-14.319551	1.051008
-52.004097	-1.058164	1.056013
-52.418313	-0.325039	1.061018
-52.129617	-12.287163	1.066022
-52.726811	-0.031677	1.071027
-52.708633	-5.491449	1.076032
-52.767733	-8.816219	1.081037
-52.655301	-6.161647	1.086042
-53.599704	-13.011194	1.091046
-54.141913	-10.514898	1.096051
-54.281644	-1.506323	1.101056
-54.635750	-1.669926	1.106061
-54.384941	-10.909666	1.111066
-54.586324	-8.892425	1.116070
-54.492445	-6.425583	1.121075
-54.635264	-10.484210	1.126080
-55.326943	-0.223762	1.131085
-55.629483	-1.614158	1.136090
-55.560473	-14.546434	1.141094
-56.518616	-0.714307	1.146099
-57.027591	-14.824185	1.151104
-57.461434	-3.679009	1.156109
-57.186620	-0.695924	1.161114
-57.373822	-5.928886	1.166118
-57.782866	1.535683	1.171123
-57.354789	-0.356653	1.176128
-57.815707	-0.306482	1.181133
-57.644019	-2.384927	1.186138
-58.230549	0.136946	1.191142
-58.706263	7.901986	1.196147
-58.768710	-10.492216	1.201152
-58.874902	-4.973125	1.206157
-59.897546	-8.811175	1.211162
-60.626472	-19.939206	1.216166
-60.240946	-13.007574	1.221171
-59.605534	-15.707024	1.226176
-60.309830	-1.006477	1.231181
-60.819893	-6.096701	1.236186
-60.817051	-9.904453	1.241190
-61.237630	1.141754	1.246195
-61.864351	-1.767599	1.251200
-62.185670	1.333539	1.256205
-62.651396	-3.780686	1.261210
-62.597578	-2.171919	1.266214
-62.322302	-5.497098	1.271219
-62.473301	-9.141311	1.276224
-62.596252	2.270152	1.281229
-62.675547	-10.259381	1.286234
-63.745947	-2.134734	1.291238
-64.293254	-3.854627	1.296243
-64.095155	1.042284	1.301248
-64.265057	-2.735441	1.306253
-64.521310	-12.205098	1.311258
-63.979585	-12.222665	1.316262
-64.936942	-3.026089	1.321267
-65.028233	-5.689691	1.326272
-65.684538	1.076631	1.331277
-65.798473	-11.400612	1.336282
-65.725538	-7.426538	1.341286
-66.033616	-9.349731	1.346291
-66.981809	-14.339329	1.351296
-67.549465	-3.436036	1.356301
-67.532192	-5.289978	1.361306
-66.974669	-0.802687	1.366310
-67.105953	1.498438	1.371315
-67.107055	-14.398621	1.376320
-67.812401	-0.139768	1.381325
-68.385650	-0.581365	1.386330
-68.651434	-9.347431	1.391334
-69.007616	-6.480161	1.396339
-68.851243	-11.268052	1.401344
-69.286511	-5.271650	1.406349
-69.142876	-8.346000	1.411354
-69.966264	-0.343859	1.416358
-70.737088	-3.236499	1.421363
-70.860051	-9.383246	1.426368
-70.844040	4.424526	1.431373
-70.644092	6.507047	1.436378
-70.711325	-7.666171	1.441382
-71.160686	-3.329747	1.446387
-71.109568	-4.348164	1.451392
-71.888683	4.689231	1.456397
-72.285802	-0.424889	1.461402
-71.984663	0.522475	1.466406
-72.428771	2.979477	1.471411
-72.361287	-1.416674	1.476416
-72.583708	2.775405	1.481421
-73.120922	-3.323107	1.486426
-73.454628	3.230774	1.491430
-73.762014	0.280583	1.496435
-73.902235	2.702556	1.501440
-74.647366	4.388807	1.506445
-75.339185	-5.317949	1.511450
-74.417168	-10.254967	1.516454
-75.249663	-1.523261	1.521459
-75.093340	0.148573	1.526464
-75.555966	-0.976229	1.531469
-75.413382	-9.179487	1.536474
-75.785096	3.815236	1.541478
-76.512148	1.142265	1.546483
-76.681694	-5.393963	1.551488
-77.082542	1.233954	1.556493
-77.121084	0.182606	1.561498
-77.208070	-11.871327	1.566502
-77.466314	3.127921	1.571507
-77.312091	-0.333520	1.576512
-78.143875	0.309094	1.581517
-78.363119	10.249869	1.586522
-78.711786	-11.984754	1.591526
-79.024545	1.213412	1.596531
-78.887102	4.951109	1.601536
-79.051763	2.846467	1.606541
-79.491482	-0.359069	1.611546
-79.905425	1.181687	1.616550
-80.320590	-2.458330	1.621555
-80.222558	4.405099	1.626560
-80.580997	-0.779733	1.631565
-80.836982	3.450350	1.636570
-80.482708	-5.479160	1.641574
-81.529242	1.182958	1.646579
-81.824373	-8.802741	1.651584
-82.040275	7.270654	1.656589
-82.154928	2.293249	1.661594
-82.267417	-5.644406	1.666598
-82.240904	-1.997489	1.671603
-82.411854	-5.117712	1.676608
-83.317290	2.614955	1.681613
-83.700592	2.182119	1.686618
-83.640286	-4.451386	1.691622
-83.800079	-0.495969	1.696627
-83.819973	-13.174119	1.701632
-84.013069	-1.920061	1.706637
-84.537771	4.409775	1.711642
-84.729953	-6.181012	1.716646
-85.279398	17.500708	1.721651
-85.659410	0.261928	1.726656
-85.751488	0.085110	1.731661
-85.499589	7.507336	1.736666
-85.503654	-2.618316	1.741670
-86.410763	-1.597643	1.746675
-86.542079	2.372305	1.751680
-86.961026	-9.898260	1.756685
-87.055375	6.475767	1.761690
-86.901477	-2.898603	1.766694
-87.738006	-2.667871	1.771699
-88.102889	-3.820170	1.776704
-88.228688	-0.214967	1.781709
-88.511258	-2.999869	1.786714
-88.806598	7.168544	1.791718
-88.749188	-5.309987	1.796723
-88.692365	-8.266897	1.801728
-89.027258	-0.826422	1.806733
-90.009748	-1.929430	1.811738
-90.097027	-2.019930	1.816742
-90.123651	4.132389	1.821747
-90.033373	-3.800204	1.826752
-90.387138	-4.526284	1.831757
-90.564087	-9.413283	1.836762
-90.981615	-12.309356	1.841766
-91.723103	6.987579	1.846771
-91.663211	-11.489280	1.851776
-91.993632	-4.103214	1.856781
-92.019375	1.992627	1.861786
-91.919626	-9.422805	1.866790
-92.706427	-2.661060	1.871795
-92.990484	0.653720	1.876800
-93.222469	1.475805	1.881805
-93.963271	-0.710996	1.886810
-93.712098	0.119926	1.891814
-94.218797	-11.191528	1.896819
-93.947558	-6.559755	1.901824
-94.006702	-2.281507	1.906829
-94.080167	4.192566	1.911834
-94.527650	1.622261	1.916838
-95.427839	-2.333885	1.921843
-95.414406	0.029643	1.926848
-95.502481	1.468697	1.931853
-95.727664	-5.452552	1.936858
-95.723328	-11.364231	1.941862
-96.715244	-3.239925	1.946867
-96.913197	-12.097500	1.951872
-97.099650	-7.369269	1.956877
-96.933532	-9.059678	1.961882
-96.776914	-10.421284	1.966886
-96.924680	-5.810727	1.971891
-97.922296	-12.057084	1.976896
-98.430082	-2.201812	1.981901
-98.477738	1.613038	1.986906
-98.341477	-1.833102	1.991910
-98.265332	11.002568	1.996915
-99.159187	-7.343143	2.006912
-99.054848	-0.241061	2.016909
-98.446059	-3.510390	2.026906
-97.997302	-8.524683	2.036902
-97.252393	-6.456927	2.046899
-96.927211	-1.718096	2.056896
-96.373886	-8.001357	2.066893
-95.926383	-2.625118	2.076890
-95.053521	2.921452	2.086886
-94.629550	-7.097711	2.096883
-94.361074	-2.216354	2.106880
-94.071025	-1.212597	2.116877
-93.145496	-3.589496	2.126874
-93.033984	-1.427083	2.136870
-92.122477	-6.558405	2.146867
-91.521765	-3.153295	2.156864
-91.443903	2.621172	2.166861
-91.060687	5.871881	2.176858
-90.165039	-4.021998	2.186854
-90.077636	-4.059275	2.196851
-89.138509	-5.400642	2.206848
-88.438335	0.486513	2.216845
-88.469731	6.795261	2.226842
-87.824081	2.149469	2.236838
-86.870594	-2.364702	2.246835
-86.671754	-3.511169	2.256832
-86.712919	2.713352	2.266829
-85.780067	-4.137002	2.276826
-85.215008	-0.135198	2.286822
-84.988289	-3.186990	2.296819
-83.701648	-9.567539	2.306816
-83.643746	-3.634987	2.316813
-83.528554	1.602617	2.326810
-82.941530	2.744580	2.336806
-82.264426	-4.231235	2.346803
-81.947480	-2.334511	2.356800
-80.907078	-2.441176	2.366797
-80.507680	-8.946588	2.376794
-80.114452	-6.262752	2.386790
-80.169408	-8.595895	2.396787
-79.179979	-12.923480	2.406784
-78.886557	-11.228182	2.416781
-78.120584	-1.414449	2.426778
-77.276122	-8.879715	2.436774
-76.977795	-3.088542	2.446771
-77.293065	-3.794882	2.456768
-76.393209	0.851743	2.466765
-75.744356	1.186584	2.476762
-75.536255	-0.367497	2.486758
-74.142453	0.501410	2.496755
-74.057576	4.943220	2.506752
-73.954543	3.003334	2.516749
-73.404777	-0.656692	2.526746
-72.731240	-7.453570	2.536742
-72.561419	-7.504714	2.546739
-71.401317	-1.931133	2.556736
-71.017397	-1.278937	2.566733
-71.085299	-2.729272	2.576730
-70.357621	5.936952	2.586726
-69.691004	0.518993	2.596723
-69.327915	-2.796309	2.606720
-68.117446	-2.593301	2.616717
-68.064743	-4.941619	2.626714
-68.037557	-11.687288	2.636710
-67.635228	-6.742261	2.646707
-66.412437	-8.063878	2.656704
-66.435329	-6.482796	2.666701
-65.558036	-3.418495	2.676698
-64.717031	-5.232750	2.686694
-64.947685	-5.801102	2.696691
-64.658965	4.814528	2.706688
-63.380984	-2.940195	2.716685
-63.209566	-2.835580	2.726682
-63.129443	-3.667669	2.736678
-61.872696	-11.247842	2.746675
-61.604542	-8.040743	2.756672
-61.489498	-3.195813	2.766669
-60.248938	-9.281640	2.776666
-60.064129	-3.370357	2.786662
-59.957002	-5.576043	2.796659
-59.222424	-3.932017	2.806656
-58.554260	-2.502233	2.816653
-58.462135	-1.667325	2.826650
-57.800932	-5.696038	2.836646
-56.987773	0.322595	2.846643
-56.940265	-1.994639	2.856640
-55.891741	-10.014543	2.866637
-55.330499	0.560741	2.876634
-55.225849	-2.371308	2.886630
-55.273642	-4.684645	2.896627
-54.225704	1.966692	2.906624
-53.735986	-1.703610	2.916621
-52.737372	-0.665818	2.926618
-52.970512	-2.616674	2.936614
-52.308674	-1.331544	2.946611
-51.454081	0.537968	2.956608
-50.590479	-2.911760	2.966605
-50.738098	-4.294543	2.976602
-50.289833	-1.652347	2.986598
-49.862822	-1.223302	2.996595
-48.837261	0.482628	3.006592
-48.598836	1.218237	3.016589
-48.560297	-2.072964	3.026586
-47.782150	2.148828	3.036582
-47.484253	-3.495888	3.046579
-46.303865	-2.625242	3.056576
-45.945006	-4.419674	3.066573
-45.667609	1.949663	3.076570
-45.646858	-4.966231	3.086566
-44.540995	-5.304727	3.096563
-44.304069	-8.212554	3.106560
-43.221878	-2.127895	3.116557
-42.900658	1.887591	3.126554
-42.744731	-2.041271	3.136550
-42.612725	-4.786998	3.146547
-41.427921	-4.312940	3.156544
-40.922669	-10.813027	3.166541
-40.774700	-8.604977	3.176538
-40.427360	-5.094769	3.186534
-39.745424	-2.329189	3.196531
-39.173559	-9.049057	3.206528
-38.379178	2.500687	3.216525
-38.262843	-0.990904	3.226522
-38.047938	-5.740938	3.236518
-36.775119	-8.255530	3.246515
-36.374130	-1.809320	3.256512
-36.244669	-1.011203	3.266509
-35.786055	-6.626322	3.276506
-35.121053	-2.989671	3.286502
-34.741511	-5.027013	3.296499
-33.916504	-7.988267	3.306496
-33.302200	-4.374600	3.316493
-32.844411	-6.166267	3.326490
-33.042240	-4.983990	3.336486
-32.112348	0.136711	3.346483
-31.590125	-10.261309	3.356480
-31.445636	-3.087920	3.366477
-30.496502	-0.051686	3.376474
-29.962690	-1.424398	3.386470
-29.570702	5.396493	3.396467
-28.981435	5.982554	3.406464
-28.189544	-7.601425	3.416461
-28.011019	0.520108	3.426458
-28.084932	-0.013399	3.436454
-27.195694	-3.862728	3.446451
-26.800357	-0.505211	3.456448
-26.243260	-0.636011	3.466445
-25.264806	1.890467	3.476442
-25.008829	-4.064800	3.486438
-24.787646	-3.571907	3.496435
-23.960200	-7.755269	3.506432
-23.284952	2.041813	3.516429
-23.183153	-10.310281	3.526426
-23.158754	-4.499318	3.536422
-22.175459	0.326099	3.546419
-21.515600	-3.055235	3.556416
-20.520096	-1.183421	3.566413
-20.676542	0.038987	3.576410
-19.967718	9.099358	3.586406
-20.210542	1.419246	3.596403
-18.973918	-1.934670	3.606400
-18.514252	-2.510027	3.616397
-18.355002	2.969423	3.626394
-17.197440	4.303322	3.636390
-16.995071	-3.990190	3.646387
-16.810421	2.556131	3.656384
-15.843502	-1.216046	3.666381
-15.552642	-5.563560	3.676378
-15.485810	-2.716824	3.686374
-14.430070	-1.111148	3.696371
-13.708936	-5.380167	3.706368
-14.013029	-6.226105	3.716365
-13.068305	-4.847452	3.726362
-12.240473	-6.167206	3.736358
-11.934078	1.183262	3.746355
-11.876148	-2.014389	3.756352
-10.682009	-5.756302	3.766349
-10.448758	-2.704343	3.776346
-10.540536	-1.161562	3.786342
-9.317019	-10.810166	3.796339
-9.015316	-11.393151	3.806336
-9.077726	-4.391179	3.816333
-7.884749	-5.700203	3.826330
-7.432037	-8.664680	3.836326
-7.263407	-3.931234	3.846323
-6.188202	-1.317121	3.856320
-5.839086	-6.797980	3.866317
-5.800979	3.868212	3.876314
-5.311649	-2.207655	3.886310
-4.591200	2.465668	3.896307
-4.241880	3.247111	3.906304
-3.511786	13.489626	3.916301
-2.826213	9.848201	3.926298
-2.905061	11.488960	3.936294
-2.360269	24.035225	3.946291
-1.989013	40.267012	3.956288
-1.628554	54.283383	3.966285
-0.978687	74.006428	3.976282
-0.636797	93.262340	3.986278
-0.261545	106.648023	3.996275
0.000000	124.115909	4.001280
0.319168	130.724339	4.006285
0.291452	153.384822	4.011290
0.198139	159.328329	4.016294
0.595839	176.491270	4.021299
0.837557	168.029432	4.026304
1.181856	198.135123	4.031309
1.239880	204.275709	4.036314
1.464334	201.981836	4.041318
0.928498	197.916968	4.046323
0.892715	198.097543	4.051328
1.134310	205.494349	4.056333
1.008319	206.413858	4.061338
1.279784	208.216646	4.066342
1.357568	204.089243	4.071347
1.543901	196.542981	4.076352
1.418404	202.469625	4.081357
1.325136	205.625753	4.086362
1.372860	195.227501	4.091366
1.398138	209.241506	4.096371
1.205016	190.488629	4.101376
0.935147	200.377028	4.106381
1.317525	201.735199	4.111386
1.374624	200.961824	4.116390
0.592944	201.393420	4.121395
0.948073	208.852757	4.126400
1.000568	216.814245	4.131405
1.363279	231.178275	4.136410
1.844437	228.087463	4.141414
1.707992	233.968575	4.146419
1.685449	247.193386	4.151424
1.355992	225.339382	4.156429
1.214601	234.398293	4.161434
1.401123	240.478592	4.166438
1.319069	237.357730	4.171443
1.512457	243.591981	4.176448
1.565649	238.982165	4.181453
1.691190	249.817255	4.186458
1.670119	234.422817	4.191462
1.324337	235.705394	4.196467
1.759422	235.730416	4.201472
1.697138	242.157958	4.206477
1.579875	238.488277	4.211482
1.695787	231.286497	4.216486
1.375499	233.444566	4.221491
1.824771	239.002968	4.226496
1.529198	236.819591	4.231501
1.714956	233.183199	4.236506
1.984784	240.187051	4.241510
1.838261	242.306442	4.246515
1.961419	237.881289	4.251520
1.759190	239.002126	4.256525
1.900895	231.103822	4.261530
2.270376	229.776177	4.266534
1.661361	235.510647	4.271539
1.866664	234.085334	4.276544
1.675757	243.481546	4.281549
1.907967	242.551276	4.286554
1.999686	235.701842	4.291558
1.677845	237.333944	4.296563
1.887173	231.571097	4.301568
1.971849	240.350751	4.306573
1.704220	236.609138	4.311578
1.920690	230.419810	4.316582
1.830401	245.694222	4.321587
1.746111	236.524111	4.326592
1.713234	224.623228	4.331597
1.435333	250.520233	4.336602
2.057886	238.382874	4.341606
1.722792	247.300564	4.346611
1.984854	242.881855	4.351616
2.008577	240.061181	4.356621
1.877418	242.731685	4.361626
2.201637	239.613039	4.366630
1.436936	246.140284	4.371635
2.104841	235.656288	4.376640
2.253242	245.282232	4.381645
1.669480	244.899774	4.386650
2.252980	234.040337	4.391654
2.001527	243.372069	4.396659
2.409960	246.838339	4.401664
2.159047	236.159212	4.406669
2.157164	249.266861	4.411674
2.220053	241.479344	4.416678
1.913801	242.521478	4.421683
1.887686	244.844524	4.426688
2.209680	250.853704	4.431693
2.092406	267.352170	4.436698
2.536315	271.442692	4.441702
2.415938	265.453348	4.446707
2.234861	259.313822	4.451712
2.151622	253.669754	4.456717
1.925055	257.921584	4.461722
2.470215	270.929478	4.466726
2.303715	275.969901	4.471731
2.549329	277.920808	4.476736
2.346866	272.038058	4.481741
1.968964	269.369580	4.486746
2.324411	258.599211	4.491750
2.301555	277.254962	4.496755
2.167267	274.910163	4.501760
2.414248	273.670337	4.506765
2.270375	286.008788	4.511770
2.579870	278.972207	4.516774
2.563288	285.242357	4.521779
2.129595	281.542383	4.526784
2.224640	278.451440	4.531789
2.252068	285.050337	4.536794
2.340591	280.485872	4.541798
1.636473	280.141258	4.546803
2.331194	281.326474	4.551808
2.419670	286.748587	4.556813
2.332531	283.815015	4.561818
2.301355	295.564919	4.566822
2.362288	297.299710	4.571827
2.537991	314.496137	4.576832
2.722453	311.865338	4.581837
2.509941	316.570649	4.586842
2.531890	314.839411	4.591846
2.485722	310.282003	4.596851
2.655996	313.635025	4.601856
2.532948	315.850188	4.606861
2.525032	316.187560	4.611866
2.778452	309.830694	4.616870
2.872034	317.273028	4.621875
3.115008	321.626143	4.626880
2.857098	317.389134	4.631885
2.465382	314.857793	4.636890
2.801023	316.025696	4.641894
2.513271	337.972736	4.646899
2.758284	319.404986	4.651904
2.802013	319.698997	4.656909
2.538047	319.200254	4.661914
2.549093	313.518189	4.666918
2.423421	316.990360	4.671923
2.696383	310.770750	4.676928
2.574997	305.670738	4.681933
2.517108	324.308756	4.686938
2.904145	313.336312	4.691942
2.398260	318.740046	4.696947
2.568412	314.600506	4.701952
2.718907	327.130274	4.706957
2.986961	345.461601	4.711962
3.372063	339.180138	4.716966
2.778566	344.745750	4.721971
2.839001	323.245673	4.726976
2.993752	327.408265	4.731981
2.719584	327.015190	4.736986
2.936377	336.490193	4.741990
2.914910	360.398040	4.746995
2.766819	349.540145	4.752000
3.082528	352.441766	4.757005
3.007883	360.643452	4.762010
3.263669	353.101323	4.767014
3.001232	361.000982	4.772019
3.115333	352.388668	4.777024
3.021551	355.200899	4.782029
3.407672	357.931753	4.787034
3.587036	340.316396	4.792038
2.378954	336.202760	4.797043
3.057616	339.173341	4.802048
3.368179	348.593393	4.807053
2.878074	362.231887	4.812058
3.118637	347.048927	4.817062
3.147470	359.995324	4.822067
3.160594	364.758565	4.827072
3.250909	357.639880	4.832077
3.028545	365.915506	4.837082
3.204415	355.352129	4.842086
2.941274	361.920744	4.847091
3.066028	372.030043	4.852096
3.070160	356.353010	4.857101
3.023360	363.947705	4.862106
3.364486	364.163271	4.867110
2.843187	359.974413	4.872115
3.238654	361.658071	4.877120
3.374552	362.880691	4.882125
3.343316	360.967141	4.887130
3.472943	347.541419	4.892134
3.006254	355.768329	4.897139
3.106079	359.029809	4.902144
3.182034	373.028683	4.907149
3.419160	387.362114	4.912154
3.670784	385.967313	4.917158
3.583713	392.205253	4.922163
3.496667	375.056721	4.927168
3.758894	359.515896	4.932173
3.592606	363.433610	4.937178
3.555296	360.327724	4.942182
3.261671	358.546622	4.947187
3.556991	361.953771	4.952192
3.406905	356.515557	4.957197
3.457699	354.741368	4.962202
3.266520	356.229458	4.967206
3.286714	373.150652	4.972211
3.541727	386.132600	4.977216
3.572527	387.302545	4.982221
3.593601	386.097871	4.987226
3.720799	392.824858	4.992230
3.601295	387.910671	4.997235
3.642837	380.801910	5.002240
3.715261	390.555237	5.007245
3.245208	392.522712	5.012250
4.041388	384.250100	5.017254
3.678264	397.088654	5.022259
3.509291	382.363718	5.027264
3.629338	384.253209	5.032269
3.727632	391.113027	5.037274
3.868429	384.592918	5.042278
3.618433	394.593092	5.047283
3.502667	390.251182	5.052288
3.898582	394.937560	5.057293
3.529049	397.814507	5.062298
3.831506	388.650340	5.067302
3.819950	394.182942	5.072307
3.701403	385.579953	5.077312
4.037386	387.352073	5.082317
3.997695	395.531230	5.087322
3.834949	386.724322	5.092326
3.727636	384.608370	5.097331
3.851770	390.381366	5.102336
4.139910	388.037577	5.107341
3.655919	386.971812	5.112346
3.885739	389.346999	5.117350
3.840536	390.682913	5.122355
3.836227	387.474491	5.127360
4.077592	391.709308	5.132365
4.092815	388.972982	5.137370
4.205855	394.123223	5.142374
4.110782	396.651645	5.147379
3.965074	386.499115	5.152384
3.876305	388.433769	5.157389
3.774481	384.239316	5.162394
3.938973	387.397280	5.167398
3.832578	392.848477	5.172403
3.964182	391.940151	5.177408
4.155722	393.620419	5.182413
3.918513	397.999733	5.187418
4.007238	384.813861	5.192422
3.754193	395.754138	5.197427
3.863286	388.971219	5.202432
4.030102	392.287636	5.207437
3.750304	400.262301	5.212442
4.245734	421.456037	5.217446
3.961405	424.139848	5.222451
4.080908	420.777082	5.227456
4.533254	422.488147	5.232461
4.065888	428.218123	5.237466
4.307711	430.799596	5.242470
4.122825	432.347721	5.247475
4.339033	424.640830	5.252480
4.434676	430.719747	5.257485
4.122389	433.382332	5.262490
4.245365	420.279560	5.267494
4.210215	434.211611	5.272499
4.319111	419.892073	5.277504
4.347992	430.847248	5.282509
4.101636	435.329996	5.287514
4.114880	425.197344	5.292518
4.448447	431.272854	5.297523
4.105627	425.180609	5.302528
4.506348	423.225462	5.307533
4.085452	427.637606	5.312538
4.245041	417.113775	5.317542
4.238751	428.901893	5.322547
4.386915	426.413613	5.327552
4.114763	421.043298	5.332557
3.811397	433.219001	5.337562
4.334413	435.967301	5.342566
4.613482	451.046707	5.347571
4.746809	462.562967	5.352576
4.523646	442.620215	5.357581
4.521557	466.594380	5.362586
4.561991	453.008880	5.367590
4.614903	448.185063	5.372595
4.637147	448.245951	5.377600
4.743387	435.072137	5.382605
4.426229	439.354969	5.387610
4.379664	431.080719	5.392614
4.514636	449.860357	5.397619
4.853494	445.200707	5.402624
4.777834	461.017103	5.407629
4.549103	445.671370	5.412634
4.683524	442.575762	5.417638
4.501850	460.208475	5.422643
4.592401	469.525262	5.427648
4.646994	459.915638	5.432653
4.293780	466.213374	5.437658
4.710281	457.623147	5.442662
4.433682	463.786578	5.447667
4.314184	464.779811	5.452672
4.625529	453.345929	5.457677
4.058247	463.486187	5.462682
4.261485	464.236568	5.467686
4.620545	472.627786	5.472691
4.861437	483.497648	5.477696
4.838496	490.606723	5.482701
4.782875	509.006927	5.487706
4.976988	497.194997	5.492710
5.181374	499.404912	5.497715
4.903626	507.469565	5.502720
5.195812	492.120179	5.507725
4.902172	486.039316	5.512730
4.946158	479.545624	5.517734
4.467733	478.839522	5.522739
4.673528	487.870607	5.527744
5.051900	492.911526	5.532749
4.748297	497.448641	5.537754
5.134125	493.752192	5.542758
5.260938	494.027249	5.547763
4.985389	496.361067	5.552768
5.173981	498.350727	5.557773
4.893983	493.511074	5.562778
4.971403	502.572755	5.567782
5.096882	505.988864	5.572787
4.747982	494.073699	5.577792
5.237622	500.854293	5.582797
4.822760	508.435102	5.587802
5.264195	490.536825	5.592806
4.766809	506.243010	5.597811
4.710367	500.299243	5.602816
5.133892	504.577192	5.607821
5.049441	506.685572	5.612826
4.917821	503.814063	5.617830
4.878175	496.889637	5.622835
5.021630	498.339705	5.627840
5.296085	500.739202	5.632845
4.945585	506.121565	5.637850
5.394205	500.847282	5.642854
5.286876	507.390703	5.647859
5.221829	510.165460	5.652864
5.373833	501.541176	5.657869
5.104963	504.468890	5.662874
5.105070	494.089453	5.667878
5.271364	512.272546	5.672883
5.466423	522.377528	5.677888
5.670614	519.926639	5.682893
4.923882	516.157187	5.687898
5.050787	515.653038	5.692902
5.496301	524.680935	5.697907
5.549777	527.639342	5.702912
5.194712	523.624622	5.707917
5.414950	529.484293	5.712922
5.690884	536.681922	5.717926
5.503925	536.570696	5.722931
5.519856	531.642764	5.727936
5.627476	518.297580	5.732941
5.234873	517.581043	5.737946
5.230164	520.735919	5.742950
5.219425	519.111874	5.747955
5.357809	525.207344	5.752960
5.660440	529.217990	5.757965
5.486373	536.761980	5.762970
5.633453	522.803433	5.767974
5.416688	523.072818	5.772979
5.498454	535.464649	5.777984
5.793009	531.401966	5.782989
6.039546	534.040984	5.787994
5.667648	523.861615	5.792998
5.536738	517.515888	5.798003
5.591097	525.373638	5.803008
5.404017	515.689672	5.808013
5.205427	526.644917	5.813018
5.567797	524.745819	5.818022
5.450653	533.046569	5.823027
5.248825	540.111434	5.828032
5.485071	525.556173	5.833037
5.542535	521.352526	5.838042
5.783483	524.462762	5.843046
5.520731	519.559478	5.848051
5.388683	524.373988	5.853056
5.644137	541.809066	5.858061
5.660299	556.043912	5.863066
5.469737	562.671158	5.868070
6.007589	562.460477	5.873075
5.995129	560.885843	5.878080
5.896613	567.989093	5.883085
5.445403	570.345934	5.888090
5.750758	556.636454	5.893094
6.073814	568.565496	5.898099
5.560916	558.193346	5.903104
5.804348	556.100307	5.908109
5.358648	566.580835	5.913114
5.520296	563.815742	5.918118
5.779390	564.701726	5.923123
5.689055	568.367105	5.928128
5.799185	566.893166	5.933133
5.371639	576.737521	5.938138
5.872354	582.254793	5.943142
6.123686	587.864679	5.948147
6.122467	597.246925	5.953152
6.116883	592.290564	5.958157
5.865417	596.515622	5.963162
6.250697	596.692917	5.968166
5.880255	597.581122	5.973171
5.901686	588.637802	5.978176
6.274497	594.912494	5.983181
6.115235	602.414804	5.988186
6.169117	590.843712	5.993190
5.881488	599.163496	5.998195
5.901690	599.759444	6.003200
6.008540	589.979996	6.008205
6.071275	598.901601	6.013210
6.250325	599.198709	6.018214
6.076144	594.918485	6.023219
5.854302	596.961974	6.028224
6.240961	586.572068	6.033229
6.036145	593.364269	6.038234
6.189184	597.406362	6.043238
6.657535	596.946218	6.048243
6.301903	590.428345	6.053248
6.355319	598.116697	6.058253
6.159606	602.152000	6.063258
6.344804	600.650854	6.068262
6.332894	596.802273	6.073267
5.774099	582.879915	6.078272
6.186843	584.467020	6.083277
6.004168	590.817524	6.088282
6.000497	590.641084	6.093286
6.137359	600.800821	6.098291
5.932597	602.235042	6.103296
6.151107	596.800353	6.108301
5.812527	599.792288	6.113306
6.218174	596.777419	6.118310
6.098760	599.081899	6.123315
5.648175	604.807785	6.128320
6.199823	597.448292	6.133325
6.479699	605.232016	6.138330
6.240285	602.231302	6.143334
6.460748	605.994500	6.148339
6.263461	602.018898	6.153344
6.521040	584.569991	6.158349
5.875701	592.859008	6.163354
6.110339	586.499607	6.168358
5.942051	582.888393	6.173363
6.029259	599.190540	6.178368
6.077415	587.499542	6.183373
6.277416	604.672647	6.188378
6.158996	611.386945	6.193382
6.126283	600.674662	6.198387
6.065892	613.348136	6.203392
6.376875	602.787814	6.208397
5.904486	594.209341	6.213402
6.251238	590.868081	6.218406
6.034313	598.414842	6.223411
5.902779	594.131320	6.228416
6.120931	596.437336	6.233421
6.017837	608.079100	6.238426
6.262017	598.776453	6.243430
6.258305	597.062349	6.248435
6.238207	605.621959	6.253440
6.576108	586.582938	6.258445
6.052726	573.539888	6.263450
5.946904	575.561341	6.268454
6.134435	565.566328	6.273459
5.877677	570.773496	6.278464
6.025372	574.916012	6.283469
5.883161	596.725814	6.288474
6.267894	598.051570	6.293478
6.445680	598.344151	6.298483
6.227874	593.310983	6.303488
6.261467	579.855743	6.308493
6.182527	568.014297	6.313498
6.091754	569.304778	6.318502
6.411352	565.362651	6.323507
5.957157	561.204675	6.328512
5.891064	571.162240	6.333517
5.961926	577.045530	6.338522
6.280757	573.626015	6.343526
6.276938	572.874528	6.348531
5.948194	571.677432	6.353536
6.089127	577.109526	6.358541
6.071323	570.197144	6.363546
5.926245	571.723018	6.368550
6.280342	590.837963	6.373555
6.136455	588.318698	6.378560
6.133596	571.717887	6.383565
6.160462	585.086952	6.388570
6.119954	573.711817	6.393574
6.079150	573.339858	6.398579
6.268832	580.397955	6.403584
6.368979	573.257913	6.408589
5.730303	570.974618	6.413594
5.896685	571.271451	6.418598
5.983587	584.679134	6.423603
6.028179	594.061898	6.428608
6.330920	596.628400	6.433613
6.303518	601.701091	6.438618
6.483361	592.959094	6.443622
5.962277	581.874299	6.448627
5.527461	574.904054	6.453632
6.214520	588.041096	6.458637
6.257245	596.253603	6.463642
6.217044	594.168953	6.468646
6.257921	598.785022	6.473651
6.067872	588.480848	6.478656
6.642573	592.735320	6.483661
6.184013	587.192517	6.488666
6.181501	573.903862	6.493670
6.107872	569.050702	6.498675
5.987899	576.679299	6.503680
6.246558	564.150266	6.508685
6.124705	571.908807	6.513690
6.072120	574.832954	6.518694
6.211174	575.435405	6.523699
5.983576	576.602585	6.528704
6.185548	557.203273	6.533709
5.857348	567.017984	6.538714
6.142136	556.962805	6.543718
6.095455	571.413552	6.548723
6.083110	571.103879	6.553728
6.111343	568.809130	6.558733
5.869355	576.586244	6.563738
6.022736	582.507990	6.568742
6.112752	592.317436	6.573747
5.981646	601.300278	6.578752
6.424935	593.871973	6.583757
5.928142	593.801687	6.588762
6.009859	594.113992	6.593766
6.389921	599.316958	6.598771
6.018543	600.664074	6.603776
6.474687	596.468318	6.608781
6.365804	589.212163	6.613786
6.004505	578.647032	6.618790
6.344301	570.011112	6.623795
6.140238	569.104873	6.628800
6.074248	574.587341	6.633805
5.880384	571.344500	6.638810
5.849510	567.601960	6.643814
6.194264	570.326271	6.648819
6.053238	570.508654	6.653824
6.165664	578.670269	6.658829
6.037778	574.137533	6.663834
6.039113	579.170741	6.668838
6.320274	597.320943	6.673843
6.227070	588.541298	6.678848
6.023486	574.915117	6.683853
6.206515	575.899503	6.688858
6.031495	572.892495	6.693862
6.116998	565.229528	6.698867
6.049592	579.735010	6.703872
5.964527	577.493611	6.708877
6.148273	592.426223	6.713882
5.928244	597.320013	6.718886
6.390481	602.763641	6.723891
6.348183	598.896996	6.728896
6.366842	582.160219	6.733901
6.321695	581.651450	6.738906
6.072912	575.253750	6.743910
6.135367	569.085792	6.748915
6.072484	574.499377	6.753920
6.063044	566.910504	6.758925
5.631183	573.055537	6.763930
5.709033	573.789154	6.768934
5.868895	589.883253	6.773939
5.899647	602.004171	6.778944
6.144870	603.114823	6.783949
6.291146	612.767394	6.788954
6.469703	598.616523	6.793958
6.552145	599.910348	6.798963
6.452273	607.150480	6.803968
6.048858	582.669403	6.808973
6.256215	581.818891	6.813978
6.152350	582.793466	6.818982
6.532106	567.189502	6.823987
5.847678	574.891744	6.828992
5.931248	574.475061	6.833997
6.070630	572.500732	6.839002
5.741272	576.554563	6.844006
6.015171	590.194172	6.849011
5.682577	594.673261	6.854016
5.887842	601.310387	6.859021
6.250443	600.342369	6.864026
6.711207	610.738738	6.869030
6.546592	600.121161	6.874035
6.300486	594.626020	6.879040
6.258564	580.593880	6.884045
6.243834	577.182033	6.889050
6.160338	573.683484	6.894054
6.431757	566.451410	6.899059
6.030258	574.092295	6.904064
6.147523	574.282113	6.909069
6.431290	571.372530	6.914074
6.089655	569.236969	6.919078
6.292467	574.472967	6.924083
5.955026	571.101920	6.929088
6.113360	572.398887	6.934093
6.168537	577.577102	6.939098
6.377908	573.516350	6.944102
5.959377	575.296862	6.949107
5.981371	583.734175	6.954112
5.976019	575.867593	6.959117
6.248474	568.346183	6.964122
5.991396	573.396738	6.969126
6.385516	572.014185	6.974131
5.939258	562.868869	6.979136
6.232023	577.190916	6.984141
6.052895	573.850731	6.989146
5.568488	565.731536	6.994150
5.992317	573.710276	6.999155
5.685097	573.649705	7.004160
6.344630	570.756458	7.009165
5.805974	569.183835	7.014170
6.064095	573.622818	7.019174
6.292740	580.182078	7.024179
6.181166	576.043840	7.029184
6.094399	572.384528	7.034189
6.036796	572.036458	7.039194
6.044933	579.877013	7.044198
6.301766	579.072684	7.049203
6.091088	579.712705	7.054208
6.212658	565.542869	7.059213
6.049779	567.330461	7.064218
5.644667	568.132938	7.069222
6.202895	590.146433	7.074227
5.858146	595.608282	7.079232
6.305051	596.133716	7.084237
6.382520	599.844083	7.089242
6.158467	604.436847	7.094246
6.184460	599.936291	7.099251
6.148870	605.579786	7.104256
5.938737	583.802928	7.109261
5.957594	602.270256	7.114266
6.184929	597.059836	7.119270
6.410515	600.737143	7.124275
6.120822	591.230602	7.129280
6.217827	585.813727	7.134285
5.776518	586.601271	7.139290
5.918587	599.747979	7.144294
5.943378	600.587445	7.149299
6.339619	602.548427	7.154304
6.499459	594.526579	7.159309
6.378412	596.426143	7.164314
5.903934	589.414597	7.169318
5.953550	591.823936	7.174323
5.925743	592.232476	7.179328
6.159276	603.699134	7.184333
6.548621	602.834825	7.189338
6.028347	601.395999	7.194342
6.130414	583.671296	7.199347
6.073251	593.051636	7.204352
6.345955	592.189239	7.209357
6.106462	582.752248	7.214362
5.882561	573.840895	7.219366
6.168954	574.947701	7.224371
6.227225	590.153114	7.229376
6.354605	577.894578	7.234381
6.032052	568.278250	7.239386
6.037308	568.330008	7.244390
6.375883	566.661650	7.249395
6.052869	574.216855	7.254400
6.276232	567.666845	7.259405
6.184617	581.587742	7.264410
5.723189	577.834958	7.269414
5.971987	573.051046	7.274419
5.751082	585.028556	7.279424
6.055225	591.387501	7.284429
6.457518	600.971810	7.289434
6.122566	606.144163	7.294438
6.245743	602.174304	7.299443
6.043085	595.780319	7.304448
5.999352	601.606392	7.309453
6.062401	600.616448	7.314458
6.445330	610.751412	7.319462
6.334324	585.282002	7.324467
6.282165	577.804958	7.329472
6.231805	568.722469	7.334477
6.099950	570.684294	7.339482
5.917162	577.367482	7.344486
6.232021	569.569631	7.349491
5.869178	570.620053	7.354496
5.987371	568.284591	7.359501
6.463622	566.567830	7.364506
5.870260	580.390901	7.369510
6.099742	568.887689	7.374515
6.277417	583.262698	7.379520
6.256506	573.381743	7.384525
5.988762	568.685067	7.389530
5.963224	573.331736	7.394534
6.412693	563.895049	7.399539
6.003231	561.529974	7.404544
5.879407	562.678918	7.409549
6.059626	571.120167	7.414554
6.440237	591.644684	7.419558
6.340322	561.845094	7.424563
6.261220	571.680897	7.429568
6.087822	576.772379	7.434573
6.221132	568.644235	7.439578
6.170964	573.823282	7.444582
5.826774	574.441662	7.449587
5.810674	569.265462	7.454592
6.020573	564.243804	7.459597
6.004099	578.666481	7.464602
6.293468	589.178174	7.469606
6.541203	581.367141	7.474611
6.119676	575.372687	7.479616
6.268928	568.198882	7.484621
6.122660	579.363551	7.489626
6.073525	567.785527	7.494630
6.203806	563.767543	7.499635
6.099216	567.920177	7.504640
6.267882	566.516970	7.509645
6.031835	563.054486	7.514650
6.020951	571.407151	7.519654
6.135904	568.541745	7.524659
6.146527	573.895433	7.529664
6.275321	567.971738	7.534669
6.118828	575.437272	7.539674
6.113146	568.070742	7.544678
6.294691	560.108366	7.549683
5.959917	567.729737	7.554688
6.346514	559.352660	7.559693
6.245800	567.388681	7.564698
6.362165	568.621945	7.569702
5.997307	565.848161	7.574707
6.123820	576.015611	7.579712
6.050297	564.604502	7.584717
6.242910	576.657216	7.589722
6.348841	570.669324	7.594726
6.465418	567.262516	7.599731
6.252628	576.861439	7.604736
6.265343	569.128909	7.609741
6.317457	562.796722	7.614746
6.465760	569.696302	7.619750
6.424656	560.503766	7.624755
6.059761	548.030436	7.629760
5.622952	544.881121	7.634765
6.015878	561.777529	7.639770
6.126445	562.519353	7.644774
6.175685	564.379921	7.649779
6.147583	570.672514	7.654784
6.193533	563.762227	7.659789
6.400331	575.754191	7.664794
6.256892	556.083631	7.669798
6.263299	545.115221	7.674803
6.087490	536.906174	7.679808
6.069858	542.688054	7.684813
6.043110	525.977192	7.689818
5.997835	537.978227	7.694822
6.357060	533.969871	7.699827
6.168989	526.746168	7.704832
6.170830	543.007805	7.709837
5.852738	529.671696	7.714842
5.934390	539.837459	7.719846
6.477807	546.068843	7.724851
6.092006	537.283022	7.729856
5.902119	528.174188	7.734861
6.256183	549.897276	7.739866
5.992396	551.200069	7.744870
6.116390	544.391632	7.749875
6.168283	554.066867	7.754880
5.948880	552.254533	7.759885
6.277659	555.832299	7.764890
6.429499	556.893759	7.769894
6.255454	542.012249	7.774899
6.201394	539.495512	7.779904
6.146301	537.104535	7.784909
5.949256	533.722529	7.789914
6.088310	542.639875	7.794918
6.207630	538.916227	7.799923
5.811588	545.327623	7.804928
5.665452	532.942462	7.809933
5.913862	554.174835	7.814938
5.798821	574.963063	7.819942
6.246901	568.429192	7.824947
6.289599	572.203704	7.829952
6.066786	576.038371	7.834957
6.167408	572.176725	7.839962
5.889513	571.345630	7.844966
6.343079	567.854522	7.849971
6.344677	571.208838	7.854976
6.365408	574.042930	7.859981
6.499776	566.711169	7.864986
5.950479	555.351166	7.869990
6.004858	556.941550	7.874995
6.271508	569.730337	7.880000
5.924396	573.495372	7.885005
6.165630	551.063373	7.890010
5.714594	571.388876	7.895014
6.084886	572.042003	7.900019
5.810857	581.505530	7.905024
5.905519	584.435141	7.910029
6.096235	575.212772	7.915034
5.985115	577.263415	7.920038
6.001864	568.697849	7.925043
6.160821	576.247894	7.930048
6.277789	583.284563	7.935053
6.330736	582.086643	7.940058
6.058694	584.861682	7.945062
6.265022	577.093207	7.950067
6.086749	585.412670	7.955072
6.180975	575.728844	7.960077
6.280430	576.512856	7.965082
6.197766	577.352714	7.970086
6.334372	576.865409	7.975091
6.121482	584.536199	7.980096
6.026040	578.187151	7.985101
6.458761	565.976921	7.990106
6.264573	581.937336	7.995110
6.220260	561.932612	8.000115
6.098018	560.886293	8.005133
5.927275	553.206762	8.010150
6.172679	555.013614	8.015168
6.238197	570.787240	8.020186
6.228997	561.459682	8.025203
5.933564	557.177435	8.030221
6.203058	567.629642	8.035238
6.233826	567.299666	8.040256
6.189218	574.771326	8.045274
6.059764	575.680378	8.050291
6.215103	569.899218	8.055309
6.164620	574.307702	8.060326
6.129904	567.270019	8.065344
6.261583	576.598880	8.070362
6.403648	564.129923	8.075379
6.020294	559.378247	8.080397
5.986066	567.236298	8.085414
6.343214	573.456371	8.090432
5.977406	573.387561	8.095450
6.141383	573.022385	8.100467
6.384121	579.348456	8.105485
6.510605	575.970399	8.110502
6.599743	569.037814	8.115520
6.203742	561.273579	8.120538
6.448487	544.936874	8.125555
6.132849	544.147615	8.130573
5.673862	548.067313	8.135590
5.998384	550.440106	8.140608
6.083900	568.774669	8.145626
6.340670	573.621256	8.150643
6.540314	567.552516	8.155661
6.225444	579.478187	8.160678
6.359783	573.450841	8.165696
6.317443	576.847750	8.170714
6.420747	573.655475	8.175731
6.428797	568.502077	8.180749
6.245657	567.800249	8.185766
6.401272	573.247293	8.190784
5.903596	571.337362	8.195802
6.186841	566.061535	8.200819
6.236841	576.631106	8.205837
6.457029	564.481062	8.210854
6.559441	567.743736	8.215872
6.381903	572.592226	8.220890
6.260941	568.132650	8.225907
6.361144	569.478458	8.230925
6.537023	570.065061	8.235942
6.218506	568.531938	8.240960
6.116708	573.162638	8.245978
6.250050	575.664449	8.250995
6.206886	572.653730	8.256013
5.908836	569.464112	8.261030
6.020946	570.795849	8.266048
6.046174	587.472820	8.271066
6.425016	582.041651	8.276083
6.123514	573.233752	8.281101
6.221397	580.487320	8.286118
6.391746	595.035523	8.291136
6.605214	606.627695	8.296154
6.512971	597.257944	8.301171
6.504452	593.919217	8.306189
6.358633	581.018291	8.311206
6.511390	590.794963	8.316224
6.353747	589.746864	8.321242
6.881276	578.380695	8.326259
6.342861	582.201641	8.331277
6.073416	578.423751	8.336294
6.709219	589.012249	8.341312
6.451431	587.192569	8.346330
6.679444	584.084387	8.351347
6.434995	579.442794	8.356365
6.267734	568.719886	8.361382
6.473858	584.737068	8.366400
6.334879	595.930676	8.371418
6.786765	598.514273	8.376435
6.832630	581.689632	8.381453
6.051291	589.543427	8.386470
6.443939	581.379224	8.391488
6.559734	602.172403	8.396506
6.762458	598.296898	8.401523
7.032091	584.452882	8.406541
6.434968	585.020307	8.411558
6.398631	571.505353	8.416576
6.251817	571.598443	8.421594
6.674093	579.323494	8.426611
6.369473	585.608157	8.431629
6.453896	597.782361	8.436646
6.931595	591.884646	8.441664
6.602905	598.746111	8.446682
6.418822	595.326280	8.451699
6.808623	596.421813	8.456717
6.744616	593.883436	8.461734
6.518040	577.156862	8.466752
6.551764	577.770401	8.471770
6.586148	575.310630	8.476787
6.543906	581.591098	8.481805
6.547512	591.146898	8.486822
6.643981	589.377020	8.491840
6.717600	600.533531	8.496858
6.733091	602.610324	8.501875
6.800365	606.629155	8.506893
6.680358	584.291787	8.511910
6.463821	573.251691	8.516928
6.316782	591.392573	8.521946
6.494071	601.647878	8.526963
6.829423	598.459959	8.531981
6.724577	615.206084	8.536998
6.744659	611.284887	8.542016
6.622128	609.679419	8.547034
6.677146	611.530729	8.552051
6.614807	607.421816	8.557069
6.191896	604.378095	8.562087
6.420685	602.167043	8.567104
6.395392	597.283463	8.572122
6.561705	617.628344	8.577139
6.742836	607.226403	8.582157
6.690092	608.041006	8.587175
6.754790	613.571480	8.592192
6.598970	612.951535	8.597210
6.326536	612.904000	8.602227
6.699203	613.319628	8.607245
6.957388	618.097800	8.612263
6.738611	616.991606	8.617280
6.866856	617.646503	8.622298
6.716486	615.308971	8.627315
7.094066	610.356547	8.632333
6.741911	606.508279	8.637351
6.663501	610.318064	8.642368
6.407072	617.766591	8.647386
7.060756	620.724636	8.652403
7.357983	628.404346	8.657421
6.709454	628.849487	8.662439
6.842040	616.704727	8.667456
6.637287	610.462983	8.672474
6.610038	602.959675	8.677491
7.039961	617.285217	8.682509
6.644295	630.708335	8.687527
6.793971	630.635721	8.692544
7.213325	642.949652	8.697562
7.084025	634.851305	8.702579
7.208941	621.725719	8.707597
6.963008	621.245837	8.712615
6.763528	607.492018	8.717632
7.007530	603.928228	8.722650
6.551028	609.982835	8.727667
6.702652	607.119607	8.732685
6.528621	615.427964	8.737703
6.865822	630.177323	8.742720
7.116259	631.220314	8.747738
6.952908	645.042369	8.752755
7.105741	631.253629	8.757773
6.766627	621.366011	8.762791
6.918185	624.505736	8.767808
7.109635	636.277124	8.772826
6.740474	631.235538	8.777843
6.906096	634.919290	8.782861
6.898375	645.526690	8.787879
6.844192	632.888180	8.792896
7.147988	639.707039	8.797914
6.784799	651.780093	8.802931
6.939895	637.434488	8.807949
7.116609	640.424419	8.812967
7.098711	642.363555	8.817984
7.447264	649.486870	8.823002
6.932945	648.382869	8.828019
7.090006	644.141448	8.833037
6.807094	650.396669	8.838055
6.892098	648.451253	8.843072
7.140832	644.736604	8.848090
7.003275	647.552531	8.853107
7.115002	643.561762	8.858125
6.882857	645.322369	8.863143
6.712500	648.382547	8.868160
6.669082	649.106948	8.873178
6.736741	644.246960	8.878195
6.697185	638.799890	8.883213
7.113368	638.689138	8.888231
6.806404	637.676929	8.893248
6.824393	641.713263	8.898266
7.038819	634.305211	8.903283
7.268686	654.711180	8.908301
7.213767	649.090794	8.913319
7.288771	646.183047	8.918336
6.993164	644.236171	8.923354
7.021557	645.908457	8.928371
6.950331	648.403838	8.933389
7.211345	657.032176	8.938407
7.080475	677.793302	8.943424
7.360534	659.798205	8.948442
7.180025	666.433578	8.953459
7.120410	660.910106	8.958477
7.135740	656.372382	8.963495
7.396735	661.838256	8.968512
7.287833	653.460893	8.973530
6.959582	642.268277	8.978547
7.055683	649.192512	8.983565
7.411718	665.557274	8.988583
7.193019	668.003125	8.993600
7.394517	651.469163	8.998618
7.169628	665.684598	9.003635
7.227754	645.279427	9.008653
7.334003	648.153470	9.013671
7.125044	658.652823	9.018688
7.416893	641.777922	9.023706
7.191545	650.149590	9.028723
7.191969	646.021831	9.033741
7.244801	653.418875	9.038759
6.883861	661.285303	9.043776
7.605795	664.688683	9.048794
7.532296	665.683554	9.053811
7.006425	665.013659	9.058829
6.973894	657.536389	9.063847
7.110076	653.663600	9.068864
7.437407	662.950832	9.073882
6.867303	667.882134	9.078899
7.080010	659.889626	9.083917
7.075144	662.980026	9.088935
7.263624	669.998924	9.093952
7.533946	663.725886	9.098970
7.467451	666.552608	9.103987
7.420617	669.738905	9.109005
7.771696	669.525843	9.114023
7.302518	667.824929	9.119040
7.968735	660.731695	9.124058
7.498789	678.218601	9.129075
7.441541	673.734097	9.134093
7.624572	664.762824	9.139111
7.368743	672.575084	9.144128
7.537535	663.481780	9.149146
7.305406	659.474715	9.154163
7.240925	672.011117	9.159181
7.263219	670.321289	9.164199
7.282085	674.145225	9.169216
7.444925	676.941431	9.174234
7.237273	670.624862	9.179251
7.044497	670.005511	9.184269
7.386756	672.785548	9.189287
7.300353	684.558312	9.194304
7.529944	672.999033	9.199322
7.460879	683.387113	9.204339
7.420180	673.928007	9.209357
7.154105	671.103977	9.214375
6.778767	676.857359	9.219392
6.990746	685.281358	9.224410
7.699706	697.974459	9.229427
7.949015	697.378490	9.234445
7.927468	688.731996	9.239463
7.271871	690.312338	9.244480
7.845130	665.975416	9.249498
7.566843	681.333622	9.254515
7.486715	675.622429	9.259533
7.738337	672.318732	9.264551
7.554151	679.261646	9.269568
7.807389	666.332294	9.274586
7.465941	672.899894	9.279603
7.664542	680.536885	9.284621
7.335594	674.068247	9.289639
7.284928	679.711689	9.294656
7.444510	664.312766	9.299674
7.390890	671.400014	9.304691
7.281485	696.009523	9.309709
7.833977	693.565374	9.314727
7.587788	705.117165	9.319744
7.860678	705.005295	9.324762
7.525745	697.394155	9.329779
7.926226	708.314579	9.334797
7.980589	693.929576	9.339815
7.537935	696.387249	9.344832
7.696718	679.487356	9.349850
7.789509	674.197698	9.354867
7.624011	674.840129	9.359885
7.852198	673.703662	9.364903
7.602630	687.025141	9.369920
7.665970	667.652344	9.374938
7.756217	672.758719	9.379955
7.254305	677.741243	9.384973
7.741565	685.277100	9.389991
8.047716	696.825781	9.395008
7.847071	675.104738	9.400026
8.008334	677.260680	9.405043
7.418794	684.678673	9.410061
7.557836	678.068043	9.415079
7.466561	686.055637	9.420096
7.645754	688.481596	9.425114
8.076041	703.057602	9.430131
7.909118	711.919946	9.435149
7.809242	696.567213	9.440167
7.796799	692.314231	9.445184
7.665534	691.657751	9.450202
7.954937	688.540683	9.455219
7.834170	692.557350	9.460237
7.891322	683.516826	9.465255
7.801507	687.059570	9.470272
7.572292	678.955078	9.475290
7.706743	705.142887	9.480307
7.603142	706.921129	9.485325
7.830744	691.195941	9.490343
7.778227	704.110830	9.495360
7.658845	701.243167	9.500378
7.564435	704.409090	9.505395
7.455842	708.645656	9.510413
7.984117	690.251109	9.515431
7.692305	710.627341	9.520448
8.081280	702.929536	9.525466
7.994573	704.313329	9.530483
7.821252	708.513159	9.535501
7.859525	711.169456	9.540519
7.611102	705.367583	9.545536
8.263944	706.896927	9.550554
8.067254	715.076135	9.555571
7.946470	697.901519	9.560589
8.113455	708.775605	9.565607
8.160148	707.607821	9.570624
8.245547	701.234742	9.575642
8.148767	705.917595	9.580659
7.743344	701.735160	9.585677
7.985180	700.178800	9.590695
7.829987	706.424550	9.595712
7.653794	710.350203	9.600730
8.214574	696.146912	9.605747
7.559772	701.307239	9.610765
7.712603	701.241877	9.615783
7.922646	703.668054	9.620800
8.009076	703.550193	9.625818
7.711224	704.523295	9.630835
7.668787	718.116911	9.635853
7.829600	729.568299	9.640871
7.874122	736.952192	9.645888
7.920011	725.994776	9.650906
8.170000	741.438150	9.655923
7.968808	738.095116	9.660941
8.190185	740.577092	9.665959
8.100826	741.193363	9.670976
7.794551	734.509575	9.675994
8.216757	743.461947	9.681011
8.056712	747.487284	9.686029
7.846097	741.830105	9.691047
8.175794	738.441359	9.696064
8.031506	746.191040	9.701082
8.312176	745.298898	9.706099
8.283840	741.037310	9.711117
8.321746	738.027134	9.716135
8.248174	747.267304	9.721152
8.024639	744.436132	9.726170
8.281794	734.186077	9.731187
7.998111	742.563892	9.736205
8.065859	741.080285	9.741223
8.081933	741.796531	9.746240
8.014263	741.456151	9.751258
8.167296	735.662812	9.756275
7.651629	742.340810	9.761293
8.121557	749.817863	9.766311
8.477553	760.024159	9.771328
8.169638	756.461203	9.776346
8.666574	751.574231	9.781363
7.976198	741.874675	9.786381
8.369333	748.135124	9.791399
8.097292	742.223185	9.796416
8.084222	747.374802	9.801434
8.711368	764.229609	9.806451
8.189060	756.401518	9.811469
8.243629	753.030386	9.816487
8.222961	752.783498	9.821504
8.412859	761.963802	9.826522
8.662535	762.567641	9.831539
8.510920	747.758051	9.836557
8.328716	738.136301	9.841575
8.403728	738.408835	9.846592
8.137153	732.989505	9.851610
8.377289	739.273658	9.856627
7.918277	739.235601	9.861645
8.457556	750.114421	9.866663
8.647036	758.492286	9.871680
8.617191	752.848037	9.876698
8.484504	735.360838	9.881715
8.007132	737.935553	9.886733
8.386943	743.644567	9.891751
8.342384	753.116022	9.896768
8.075580	770.696505	9.901786
8.837729	771.722057	9.906803
8.361835	767.906892	9.911821
8.845411	772.415724	9.916839
8.222726	757.943567	9.921856
8.393212	773.722984	9.926874
8.701896	773.777213	9.931891
8.281153	775.258921	9.936909
8.304330	774.304920	9.941927
8.501466	774.751922	9.946944
8.594128	769.019816	9.951962
8.539187	780.661198	9.956979
8.202512	784.302918	9.961997
8.258949	773.156358	9.967015
8.310171	782.672721	9.972032
8.868325	781.865012	9.977050
8.877748	770.005789	9.982067
8.436825	778.929786	9.987085
8.475813	780.980480	9.992103
8.563891	775.175227	9.997120
8.729241	782.465763	10.002138
8.794086	774.852288	10.007155
8.575162	773.328173	10.012173
8.575986	774.816383	10.017191
8.974617	781.364760	10.022208
8.788864	774.567847	10.027226
8.637493	761.780558	10.032243
8.539800	765.134403	10.037261
8.901748	759.783114	10.042279
8.883731	755.201274	10.047296
8.452322	747.794895	10.052314
8.422607	740.359434	10.057331
8.383779	749.122397	10.062349
8.543024	761.833770	10.067367
8.696386	775.162742	10.072384
8.365490	774.035505	10.077402
8.820009	777.264737	10.082419
9.070255	773.176649	10.087437
8.969937	781.464549	10.092455
8.613612	773.080871	10.097472
8.282259	782.217921	10.102490
8.634315	768.563034	10.107507
8.511685	782.420896	10.112525
8.393746	768.751273	10.117543
8.298291	776.851001	10.122560
8.293677	783.388276	10.127578
8.230993	780.439194	10.132595
8.427624	795.370278	10.137613
8.578055	808.354257	10.142631
8.874518	813.366474	10.147648
8.845045	812.262145	10.152666
8.694838	812.229246	10.157683
8.290536	809.058613	10.162701
8.641421	808.345577	10.167719
9.087147	807.348808	10.172736
8.844265	806.549381	10.177754
8.969768	801.788820	10.182771
8.773047	807.621276	10.187789
8.930522	812.646325	10.192807
9.030723	811.604214	10.197824
9.116470	810.927317	10.202842
9.098633	802.562279	10.207859
9.149126	811.589206	10.212877
8.949176	812.902369	10.217895
9.116703	806.046667	10.222912
8.837806	822.008348	10.227930
9.057567	812.741897	10.232947
9.093315	806.940753	10.237965
8.883722	814.728322	10.242983
9.025076	815.143802	10.248000
9.011455	815.547105	10.253018
9.152309	808.425978	10.258035
8.730766	793.409915	10.263053
8.922440	809.790380	10.268071
9.144546	801.279019	10.273088
8.716728	812.200693	10.278106
8.998285	809.648080	10.283123
9.059655	809.852115	10.288141
9.052385	814.190644	10.293159
9.097325	816.795474	10.298176
9.217014	813.187723	10.303194
9.294721	817.034248	10.308211
9.101196	796.966471	10.313229
8.993279	794.115593	10.318247
9.161815	787.006729	10.323264
8.816775	787.846617	10.328282
8.941419	804.966266	10.333299
8.926626	805.071491	10.338317
8.662193	813.953648	10.343335
9.231918	801.996002	10.348352
8.825880	810.866525	10.353370
8.966373	819.127050	10.358387
9.180163	820.982949	10.363405
9.197452	812.679412	10.368423
9.325082	810.119859	10.373440
9.251874	813.065806	10.378458
9.353404	805.544266	10.383475
9.213844	811.392371	10.388493
8.944308	812.851753	10.393511
9.325349	812.233321	10.398528
8.949717	824.645806	10.403546
9.220688	819.467868	10.408563
9.087653	822.768915	10.413581
9.056694	813.865588	10.418599
9.161901	813.055873	10.423616
8.860579	815.295954	10.428634
8.752133	805.429930	10.433651
8.899910	818.767243	10.438669
8.938731	837.821129	10.443687
9.319481	835.889108	10.448704
9.285517	843.184466	10.453722
9.173913	845.280917	10.458739
9.149571	849.963061	10.463757
9.071206	849.078090	10.468775
9.352026	845.566910	10.473792
9.656772	851.112417	10.478810
9.387788	839.290587	10.483827
9.714121	842.917620	10.488845
9.701614	855.510925	10.493863
9.896861	830.107383	10.498880
9.565160	820.464822	10.503898
9.319469	812.116275	10.508915
9.369522	812.556291	10.513933
9.349591	813.267863	10.518951
9.211321	808.547543	10.523968
9.153624	797.243187	10.528986
9.029274	815.621582	10.534003
9.419856	823.359965	10.539021
9.086810	847.821571	10.544039
9.400925	836.778026	10.549056
9.243697	838.129399	10.554074
9.232602	849.858746	10.559091
9.353878	833.317279	10.564109
9.298228	846.990147	10.569127
9.508688	849.105115	10.574144
9.260033	856.732458	10.579162
9.647226	839.934186	10.584179
9.913354	840.978535	10.589197
9.327961	849.123936	10.594215
9.620524	850.476163	10.599232
9.480085	846.009786	10.604250
9.522135	849.484230	10.609267
9.960772	846.629522	10.614285
9.638612	856.031582	10.619303
9.919457	846.423385	10.624320
9.713878	855.784628	10.629338
9.523956	862.641877	10.634355
9.838552	849.275242	10.639373
9.481773	848.595404	10.644391
9.694690	854.965880	10.649408
9.570330	851.981808	10.654426
9.509199	845.402906	10.659443
9.668406	853.706412	10.664461
9.315667	853.925249	10.669479
9.416186	839.480424	10.674496
9.632162	845.841141	10.679514
9.637528	841.724518	10.684531
9.774780	851.228478	10.689549
9.299115	846.584371	10.694567
9.638283	843.207716	10.699584
9.670412	846.877267	10.704602
9.592584	847.889792	10.709619
9.661099	852.103033	10.714637
9.562130	860.261348	10.719655
9.669335	845.416765	10.724672
9.599297	846.909410	10.729690
9.376219	853.273898	10.734707
9.680698	848.535114	10.739725
9.670509	873.091608	10.744743
9.708060	864.875820	10.749760
9.732824	874.919646	10.754778
10.039668	876.968011	10.759795
10.211786	870.814937	10.764813
9.703733	855.260355	10.769831
9.893253	841.245622	10.774848
9.924681	851.400122	10.779866
9.683806	848.037741	10.784883
10.112302	845.552949	10.789901
9.613976	846.367688	10.794919
9.730290	835.590155	10.799936
9.858448	850.896517	10.804954
9.765416	859.948470	10.809971
10.349465	858.678196	10.814989
10.053604	861.573954	10.820007
9.737882	839.525696	10.825024
10.131828	850.464326	10.830042
9.710002	852.624147	10.835059
9.691025	843.115292	10.840077
9.724346	855.666680	10.845095
10.115692	871.822124	10.850112
10.029787	878.689941	10.855130
9.989382	873.890153	10.860147
10.321939	856.601966	10.865165
9.670027	855.138275	10.870183
9.759348	854.310223	10.875200
10.013173	873.357751	10.880218
9.693662	881.777580	10.885235
9.931411	875.888806	10.890253
9.632936	880.353021	10.895271
10.095767	878.649218	10.900288
10.296610	877.949067	10.905306
9.928649	877.939064	10.910323
10.066149	869.678611	10.915341
10.366538	876.723098	10.920359
10.307013	876.802946	10.925376
10.084578	872.778871	10.930394
9.725275	883.262186	10.935411
9.792808	886.730164	10.940429
9.703841	884.520214	10.945447
9.660648	881.231240	10.950464
9.691037	873.819142	10.955482
9.828088	885.381345	10.960499
10.306189	898.191490	10.965517
10.491998	909.580722	10.970535
10.031360	911.998397	10.975552
10.451001	903.948440	10.980570
10.143140	897.108375	10.985587
10.252049	894.359713	10.990605
9.771653	894.968477	10.995623
10.230859	909.764762	11.000640
10.208976	906.892265	11.005658
10.003532	903.287247	11.010675
10.258360	908.371522	11.015693
10.663265	901.272552	11.020711
10.390796	904.778515	11.025728
10.660941	911.065456	11.030746
10.440207	895.528794	11.035763
10.229196	882.013402	11.040781
10.305502	884.474108	11.045799
10.209304	883.965538	11.050816
10.477419	872.907525	11.055834
10.006844	887.988025	11.060851
10.754952	889.880612	11.065869
10.401896	892.011951	11.070887
10.245921	878.860628	11.075904
10.124610	874.286376	11.080922
10.156588	899.243153	11.085939
10.196310	898.746170	11.090957
10.206672	911.786841	11.095975
10.375083	910.931939	11.100992
10.648311	919.246357	11.106010
10.213460	917.847658	11.111027
10.545055	915.578045	11.116045
10.798522	916.185495	11.121063
10.310858	907.224736	11.126080
10.939420	906.311900	11.131098
10.321631	919.666974	11.136115
10.697972	906.710976	11.141133
10.845961	906.807703	11.146151
10.179394	887.823507	11.151168
10.509228	882.638477	11.156186
10.547330	900.230620	11.161203
10.538352	894.395798	11.166221
10.139324	882.908654	11.171239
10.460455	905.585779	11.176256
10.193560	905.752052	11.181274
10.376611	915.259406	11.186291
10.460424	916.236662	11.191309
10.375611	907.092619	11.196327
10.120319	916.639347	11.201344
10.490072	904.731693	11.206362
10.033016	915.122245	11.211379
10.311597	918.197446	11.216397
10.766931	934.554843	11.221415
10.503214	938.838461	11.226432
10.997680	931.960856	11.231450
10.841142	935.294840	11.236467
10.595751	933.029054	11.241485
11.119831	923.237923	11.246503
10.287912	913.736420	11.251520
10.652888	924.701442	11.256538
10.961749	936.777222	11.261555
10.809925	937.436101	11.266573
11.088960	921.479679	11.271591
10.819715	918.504874	11.276608
10.789947	919.761779	11.281626
10.379596	916.018603	11.286643
10.749544	912.271460	11.291661
10.498854	918.194062	11.296679
10.589258	927.849781	11.301696
10.930026	936.727649	11.306714
10.913115	943.391510	11.311731
11.060033	941.441730	11.316749
10.826378	924.105821	11.321767
10.672337	931.155166	11.326784
10.516378	925.476487	11.331802
10.657685	944.790193	11.336819
10.754004	937.666920	11.341837
10.900460	940.405853	11.346855
11.045239	953.024024	11.351872
10.825181	940.770286	11.356890
10.529000	951.008906	11.361907
10.884991	940.970196	11.366925
10.914082	939.990113	11.371943
10.434448	946.142455	11.376960
10.925966	938.306547	11.381978
11.022786	932.338696	11.386995
10.916066	940.114642	11.392013
11.042864	933.075885	11.397031
10.980813	938.897649	11.402048
10.941340	935.237151	11.407066
10.900950	944.451584	11.412083
10.680108	941.363480	11.417101
10.915619	943.971970	11.422119
10.747829	942.977284	11.427136
10.951634	952.946307	11.432154
11.097140	962.707981	11.437171
11.181636	966.000074	11.442189
11.343966	970.532432	11.447207
11.066430	950.287033	11.452224
11.070932	944.128663	11.457242
11.247966	942.493633	11.462259
10.887836	941.302919	11.467277
11.068018	949.734778	11.472295
10.963779	955.346433	11.477312
11.418387	962.757826	11.482330
11.292149	959.585002	11.487347
11.366837	943.280800	11.492365
10.920244	952.491511	11.497383
10.997346	947.684189	11.502400
11.137450	958.452579	11.507418
11.327088	968.509076	11.512435
11.025851	980.345810	11.517453
11.285910	986.122038	11.522471
11.075708	978.237730	11.527488
11.399890	969.814015	11.532506
11.394709	979.124208	11.537523
11.264682	989.191524	11.542541
11.147936	970.998593	11.547559
11.021379	982.988517	11.552576
11.272968	977.827014	11.557594
11.179132	975.812999	11.562611
11.215364	979.967940	11.567629
11.456655	977.010215	11.572647
11.170821	983.694522	11.577664
11.362295	971.826315	11.582682
11.487971	978.452358	11.587699
11.482785	987.610812	11.592717
11.419878	978.935367	11.597735
11.302687	986.623220	11.602752
10.995542	979.335244	11.607770
11.175968	973.197978	11.612787
11.415659	982.715302	11.617805
11.346222	969.736280	11.622823
11.222997	974.761419	11.627840
11.387193	977.741676	11.632858
11.315019	977.683679	11.637875
11.266180	984.066662	11.642893
11.385809	977.041961	11.647911
11.242144	975.706732	11.652928
11.576618	992.848302	11.657946
11.582510	1007.555547	11.662963
11.611252	991.310748	11.667981
11.559209	978.300405	11.672999
11.458279	992.618765	11.678016
11.779449	985.089380	11.683034
11.720216	979.462500	11.688051
11.675900	983.458343	11.693069
11.592896	971.413092	11.698087
11.666977	981.872091	11.703104
11.342635	969.052497	11.708122
11.577148	961.527406	11.713139
11.449801	969.130035	11.718157
11.661041	970.545801	11.723175
11.765223	992.986907	11.728192
11.471520	995.640938	11.733210
11.593989	991.969902	11.738227
11.905151	1000.403467	11.743245
12.265762	991.823451	11.748263
11.703605	984.214193	11.753280
11.675218	974.764184	11.758298
11.673333	972.699744	11.763315
11.768498	987.266648	11.768333
11.695247	973.684422	11.773351
11.689929	977.460667	11.778368
11.307108	971.086617	11.783386
11.730853	977.879802	11.788403
11.887751	1000.213307	11.793421
11.889276	1003.671259	11.798439
11.802487	997.679994	11.803456
11.666476	1008.198626	11.808474
11.430544	999.575085	11.813491
11.824356	1007.852304	11.818509
11.499018	996.380256	11.823527
11.773804	1008.239715	11.828544
11.339210	999.906636	11.833562
11.245295	1005.829541	11.838579
11.358742	1013.275687	11.843597
11.481860	1014.205713	11.848615
11.830140	1036.272251	11.853632
11.955598	1037.007437	11.858650
12.255463	1034.320682	11.863667
12.061386	1036.141762	11.868685
12.540612	1028.272118	11.873703
12.110698	1029.436620	11.878720
12.321187	1008.540909	11.883738
12.402050	1002.502748	11.888755
12.022886	1002.869531	11.893773
12.143696	1006.977143	11.898791
12.020028	1010.759668	11.903808
12.018956	1000.443468	11.908826
12.233707	1000.050211	11.913843
11.985694	1006.381979	11.918861
12.155458	993.906327	11.923879
12.043010	998.874486	11.928896
11.893168	1007.216746	11.933914
11.866386	1003.791495	11.938931
11.975412	1004.056839	11.943949
12.155069	995.896715	11.948967
11.954015	1004.141254	11.953984
11.802773	1006.310211	11.959002
12.268272	1004.242238	11.964019
12.139237	1024.609599	11.969037
12.256307	1029.438971	11.974055
12.275188	1023.988208	11.979072
11.845731	1017.282239	11.984090
12.275704	1024.373183	11.989107
12.193008	1038.342667	11.994125
12.339284	1031.305271	11.999143
12.136375	1031.352722	12.004160
12.082594	1041.713325	12.009178
12.340520	1029.825137	12.014195
12.190515	1039.690605	12.019213
12.360016	1037.346794	12.024231
12.214892	1030.085258	12.029248
12.216001	1038.640345	12.034266
12.292248	1039.116976	12.039283
12.029178	1044.969441	12.044301
12.310147	1037.572637	12.049319
12.369969	1029.434857	12.054336
12.471057	1037.261339	12.059354
12.701226	1028.505354	12.064371
12.752972	1039.305033	12.069389
12.514145	1023.420897	12.074407
12.467245	1035.479181	12.079424
12.468522	1033.569793	12.084442
12.478267	1035.419976	12.089459
12.214083	1039.451085	12.094477
12.305943	1029.672759	12.099495
12.749991	1030.754441	12.104512
12.367794	1037.788791	12.109530
12.737937	1039.015931	12.114547
12.491633	1036.853215	12.119565
12.558170	1036.410152	12.124583
12.689140	1027.357130	12.129600
12.701215	1024.561859	12.134618
12.819191	1024.349625	12.139635
12.457846	1015.903072	12.144653
12.612168	1010.553434	12.149671
12.488096	1015.107351	12.154688
12.356779	1030.796379	12.159706
13.086566	1026.323322	12.164723
12.510719	1020.468074	12.169741
12.343150	1013.712235	12.174759
13.084537	1031.704852	12.179776
12.591019	1025.382630	12.184794
12.901205	1010.251042	12.189811
12.577342	1012.653215	12.194829
12.412803	1004.019350	12.199847
12.614054	1011.159500	12.204864
12.556132	1021.413017	12.209882
12.954038	1037.847425	12.214899
12.974639	1034.417978	12.219917
12.976631	1020.097122	12.224935
12.660383	1017.662551	12.229952
12.505366	1013.106719	12.234970
12.504668	1020.251610	12.239987
12.638686	1032.743989	12.245005
12.708743	1035.580491	12.250023
12.676652	1031.104421	12.255040
12.601975	1035.476392	12.260058
12.434844	1025.506066	12.265075
12.640657	1028.446489	12.270093
12.540921	1040.155596	12.275111
12.758893	1029.939080	12.280128
12.453743	1023.611808	12.285146
13.040120	1052.168118	12.290163
12.897268	1062.043342	12.295181
13.176941	1057.248664	12.300199
13.322727	1062.760586	12.305216
12.888640	1047.112300	12.310234
12.993104	1042.486911	12.315251
12.971671	1032.709789	12.320269
12.985833	1035.844454	12.325287
13.076715	1029.782878	12.330304
12.666673	1030.668652	12.335322
12.722311	1030.784972	12.340339
13.058589	1052.055622	12.345357
12.799077	1062.725780	12.350375
13.354019	1058.828366	12.355392
13.091923	1067.351288	12.360410
13.142807	1067.811446	12.365427
13.153865	1062.407920	12.370445
13.100435	1066.493169	12.375463
13.091501	1065.697088	12.380480
13.126079	1066.773025	12.385498
13.330897	1064.841217	12.390515
13.126589	1060.148167	12.395533
13.083277	1061.664462	12.400551
13.249906	1057.451558	12.405568
13.108015	1058.531661	12.410586
12.975811	1062.005033	12.415603
13.082585	1061.535835	12.420621
12.996164	1066.313821	12.425639
13.283102	1062.476637	12.430656
13.243697	1059.829804	12.435674
13.326302	1061.681923	12.440691
13.271181	1058.438576	12.445709
12.831005	1055.366127	12.450727
13.148314	1054.329551	12.455744
12.554706	1057.994702	12.460762
12.861031	1057.487411	12.465779
13.157761	1064.816990	12.470797
13.245557	1085.445793	12.475815
13.533436	1079.227353	12.480832
13.292785	1095.777286	12.485850
13.482851	1094.979809	12.490867
13.307303	1087.869016	12.495885
13.621480	1086.153936	12.500903
13.649583	1080.291758	12.505920
13.417017	1076.774632	12.510938
13.435746	1084.315881	12.515955
13.782060	1077.462497	12.520973
13.578240	1053.203585	12.525991
13.677941	1058.347003	12.531008
13.438061	1052.829857	12.536026
13.169290	1056.789102	12.541043
13.779225	1065.927632	12.546061
13.438322	1058.411968	12.551079
13.627965	1049.481103	12.556096
13.441286	1051.577294	12.561114
13.319080	1053.779936	12.566131
13.363049	1071.578061	12.571149
13.090516	1082.193701	12.576167
13.550868	1089.683427	12.581184
13.419767	1114.138948	12.586202
13.384046	1103.036804	12.591219
14.032703	1098.496045	12.596237
13.552153	1099.960210	12.601255
13.884759	1092.338938	12.606272
13.491710	1095.393296	12.611290
13.719393	1094.233953	12.616307
13.796779	1091.868945	12.621325
13.574257	1086.056054	12.626343
14.077488	1105.952368	12.631360
13.756025	1092.432114	12.636378
13.727572	1092.652867	12.641395
14.063543	1092.856107	12.646413
13.865609	1096.531261	12.651431
14.205731	1093.475896	12.656448
13.473473	1090.248788	12.661466
13.888421	1094.266878	12.666483
13.641809	1088.580388	12.671501
14.103192	1080.631396	12.676519
13.671656	1083.289619	12.681536
14.117492	1096.504211	12.686554
14.135356	1091.796283	12.691571
14.063440	1084.486507	12.696589
13.912487	1087.011962	12.701607
14.161397	1086.713730	12.706624
14.017144	1086.905005	12.711642
13.691123	1085.235493	12.716659
14.041703	1085.319606	12.721677
13.634921	1089.078476	12.726695
13.685255	1089.095493	12.731712
13.893865	1089.076513	12.736730
13.926873	1081.046171	12.741747
14.282865	1082.661612	12.746765
14.026970	1092.316404	12.751783
14.031653	1091.147660	12.756800
14.093728	1080.076411	12.761818
13.871384	1085.000663	12.766835
14.119063	1087.684220	12.771853
13.751002	1085.261744	12.776871
14.189746	1087.365788	12.781888
14.103608	1103.677240	12.786906
13.958025	1081.156006	12.791923
14.118172	1087.084981	12.796941
14.140609	1093.475421	12.801959
14.498379	1078.996029	12.806976
14.569759	1084.297063	12.811994
14.195503	1081.688242	12.817011
14.301780	1092.023609	12.822029
14.102144	1093.490163	12.827047
14.616980	1088.307657	12.832064
14.220735	1094.287642	12.837082
13.895758	1091.834427	12.842099
14.195917	1086.474244	12.847117
14.228137	1103.087735	12.852135
14.242690	1086.167439	12.857152
14.122664	1091.288921	12.862170
13.991036	1085.273246	12.867187
14.126214	1084.363797	12.872205
13.699497	1104.609619	12.877223
14.310313	1110.022470	12.882240
14.516361	1131.435400	12.887258
14.471755	1132.359494	12.892275
14.492549	1109.493258	12.897293
14.306877	1126.495085	12.902311
14.333800	1131.991837	12.907328
14.682519	1121.655344	12.912346
14.288620	1120.410559	12.917363
14.438332	1120.134428	12.922381
14.290800	1125.293335	12.927399
14.035802	1116.836631	12.932416
14.647314	1114.497705	12.937434
14.254957	1132.773056	12.942451
14.273248	1113.539502	12.947469
14.656687	1122.385628	12.952487
14.538107	1124.676839	12.957504
14.594233	1112.888165	12.962522
14.449869	1126.488258	12.967539
14.565599	1121.863345	12.972557
14.517808	1123.466986	12.977575
14.424224	1131.597787	12.982592
14.710010	1127.915082	12.987610
14.614285	1149.180497	12.992627
14.780785	1155.853799	12.997645
15.265016	1151.098898	13.002663
15.109292	1137.560466	13.007680
14.707821	1119.389612	13.012698
14.248778	1122.405085	13.017715
14.864404	1118.140995	13.022733
14.894602	1118.834849	13.027751
14.894534	1115.134239	13.032768
14.905831	1107.136207	13.037786
14.706854	1113.026720	13.042803
15.241304	1112.748023	13.047821
15.071794	1112.758660	13.052839
14.857193	1115.679809	13.057856
14.793363	1121.962096	13.062874
14.871043	1116.600682	13.067891
14.949196	1111.958954	13.072909
14.661759	1121.861062	13.077927
14.905551	1116.556436	13.082944
15.360092	1119.457741	13.087962
14.753830	1117.716643	13.092979
14.997226	1121.468847	13.097997
14.690653	1117.610654	13.103015
14.894266	1118.943260	13.108032
14.981298	1116.641801	13.113050
14.900682	1114.854383	13.118067
14.823682	1130.084020	13.123085
15.130669	1149.157843	13.128103
15.190182	1144.840393	13.133120
15.137908	1141.430247	13.138138
15.121857	1148.226217	13.143155
15.122128	1136.992333	13.148173
14.752184	1132.633669	13.153191
15.004803	1143.149972	13.158208
14.987663	1136.599300	13.163226
14.925910	1146.594619	13.168243
15.231999	1139.749430	13.173261
15.190058	1147.643396	13.178279
14.979198	1143.461752	13.183296
15.337591	1144.792007	13.188314
14.827329	1156.173636	13.193331
15.026157	1142.739575	13.198349
14.939299	1154.558237	13.203367
15.006403	1156.606992	13.208384
15.095828	1136.959948	13.213402
15.225136	1159.464161	13.218419
15.325825	1159.762376	13.223437
15.284380	1171.851455	13.228455
15.430327	1167.868870	13.233472
15.589994	1167.347235	13.238490
15.318948	1165.176190	13.243507
15.791004	1147.124490	13.248525
15.567287	1151.732309	13.253543
15.202066	1156.807929	13.258560
15.780706	1146.210429	13.263578
15.454580	1151.555526	13.268595
15.539656	1143.922583	13.273613
15.432683	1142.665218	13.278631
15.644639	1138.057661	13.283648
15.710098	1140.685331	13.288666
15.396961	1157.459675	13.293683
15.868404	1136.187946	13.298701
15.592033	1151.657013	13.303719
15.601023	1150.663903	13.308736
15.652136	1142.481349	13.313754
15.451635	1149.086577	13.318771
15.478399	1153.068454	13.323789
15.411034	1148.274807	13.328807
15.176467	1145.552156	13.333824
15.641015	1149.883272	13.338842
15.336526	1144.781034	13.343859
15.690255	1165.304788	13.348877
15.885573	1159.104761	13.353895
15.464504	1168.871724	13.358912
16.220420	1166.466415	13.363930
15.670443	1154.421824	13.368947
15.760195	1162.675665	13.373965
15.948905	1157.555886	13.378983
15.658572	1163.867551	13.384000
15.943721	1155.090107	13.389018
15.782332	1158.907048	13.394035
15.736572	1154.720358	13.399053
15.957030	1147.442735	13.404071
15.636532	1157.660318	13.409088
15.855692	1159.050388	13.414106
15.856584	1153.416264	13.419123
15.669969	1162.750843	13.424141
15.752812	1167.275532	13.429159
15.815695	1181.622401	13.434176
15.881003	1167.248334	13.439194
15.964257	1172.904072	13.444211
15.942619	1166.150227	13.449229
16.114816	1175.999442	13.454247
16.081669	1170.408726	13.459264
15.931611	1161.205837	13.464282
16.053608	1165.115690	13.469299
15.651652	1164.746697	13.474317
16.093712	1177.946434	13.479335
15.801326	1167.904799	13.484352
15.855604	1164.660081	13.489370
15.801336	1170.013991	13.494387
15.694839	1167.238288	13.499405
15.930036	1176.872598	13.504423
15.760081	1200.848339	13.509440
16.085369	1197.620040	13.514458
16.047858	1202.312242	13.519475
16.104623	1201.840085	13.524493
16.350337	1198.892019	13.529511
15.979195	1218.678682	13.534528
16.286372	1193.277794	13.539546
15.876449	1201.628399	13.544563
16.126751	1213.903513	13.549581
16.031632	1195.483550	13.554599
15.932657	1206.995446	13.559616
16.122761	1197.529664	13.564634
16.115179	1209.680488	13.569651
16.165514	1222.140400	13.574669
16.277617	1222.374339	13.579687
16.309335	1233.847928	13.584704
16.429160	1236.900223	13.589722
16.331540	1233.755777	13.594739
16.363415	1239.566660	13.599757
16.786207	1232.827124	13.604775
16.232106	1236.918593	13.609792
16.747283	1231.228977	13.614810
16.494735	1241.390708	13.619827
16.417718	1237.180426	13.624845
16.310841	1231.311170	13.629863
16.201099	1239.353963	13.634880
16.524314	1231.610769	13.639898
16.304923	1240.192467	13.644915
16.258982	1245.532626	13.649933
16.657234	1228.911111	13.654951
16.494662	1236.594385	13.659968
16.615286	1240.988856	13.664986
16.722519	1234.563433	13.670003
16.395307	1235.648587	13.675021
16.513336	1242.061081	13.680039
16.457580	1244.244897	13.685056
16.777789	1254.297422	13.690074
16.864070	1263.505679	13.695091
16.825400	1274.580561	13.700109
16.989221	1268.724422	13.705127
16.475440	1254.638853	13.710144
16.748691	1261.178239	13.715162
16.809352	1261.663555	13.720179
16.826553	1268.330677	13.725197
17.003578	1271.662852	13.730215
17.054498	1280.525442	13.735232
16.977617	1257.284440	13.740250
17.019543	1236.699990	13.745267
16.862618	1246.036405	13.750285
17.082948	1232.891579	13.755303
16.799596	1231.175636	13.760320
16.772009	1232.158134	13.765338
17.100082	1231.733057	13.770355
16.492596	1240.772330	13.775373
16.987954	1257.613736	13.780391
16.943593	1265.186756	13.785408
16.970800	1262.754829	13.790426
17.331924	1265.059688	13.795443
17.181977	1270.522932	13.800461
17.096502	1265.248459	13.805479
17.057332	1267.669066	13.810496
17.259066	1277.275510	13.815514
17.185975	1266.160726	13.820531
17.023009	1271.088804	13.825549
17.505683	1267.427459	13.830567
17.256358	1254.357274	13.835584
17.024148	1244.549898	13.840602
17.035556	1240.213012	13.845619
17.034522	1246.270834	13.850637
17.143678	1259.745698	13.855655
16.986614	1266.580769	13.860672
17.291532	1263.589841	13.865690
17.571116	1253.995869	13.870707
17.198435	1274.036360	13.875725
17.335095	1261.314131	13.880743
17.405663	1266.570685	13.885760
17.313976	1275.813476	13.890778
17.511006	1263.671925	13.895795
17.105106	1263.850936	13.900813
17.336570	1272.444354	13.905831
17.286593	1268.583083	13.910848
17.201085	1267.347747	13.915866
17.410622	1267.685448	13.920883
17.246930	1269.565501	13.925901
17.460970	1271.696273	13.930919
17.207598	1266.990404	13.935936
17.386818	1261.574962	13.940954
17.319056	1261.847087	13.945971
17.327306	1269.154172	13.950989
17.306080	1271.028395	13.956007
17.380453	1289.343910	13.961024
17.343761	1288.646878	13.966042
17.475874	1295.736293	13.971059
17.325665	1298.725957	13.976077
17.814245	1294.572367	13.981095
17.790785	1295.364649	13.986112
17.717190	1288.680154	13.991130
17.789765	1297.756662	13.996147
17.613184	1289.651414	14.001165
17.711329	1296.996404	14.006183
17.810093	1293.035559	14.011200
17.715852	1296.255898	14.016218
17.677521	1296.446400	14.021235
17.803686	1309.677393	14.026253
17.828734	1295.998730	14.031271
17.662436	1302.146669	14.036288
18.017966	1296.496992	14.041306
18.230636	1291.929422	14.046323
17.578347	1298.171448	14.051341
17.792360	1292.526066	14.056359
17.863863	1294.771327	14.061376
17.716153	1297.004002	14.066394
17.928583	1291.684029	14.071411
17.694733	1292.495924	14.076429
17.868717	1289.429989	14.081447
17.751877	1302.323829	14.086464
17.465327	1298.111744	14.091482
17.898130	1301.733890	14.096499
17.653558	1329.640063	14.101517
17.799719	1327.091239	14.106535
18.031138	1318.365488	14.111552
18.034537	1331.267037	14.116570
18.588147	1328.934303	14.121587
18.023058	1324.619050	14.126605
18.356774	1330.485387	14.131623
18.377647	1324.888837	14.136640
18.213957	1327.562279	14.141658
18.312589	1320.769006	14.146675
17.927415	1330.223887	14.151693
17.945638	1323.855058	14.156711
18.384790	1315.944457	14.161728
18.249509	1325.508804	14.166746
18.412104	1316.885358	14.171763
18.589966	1321.665215	14.176781
18.817392	1317.076896	14.181799
18.717325	1314.925402	14.186816
18.277687	1306.550672	14.191834
18.460292	1301.110841	14.196851
18.148742	1305.901501	14.201869
18.427557	1318.374121	14.206887
18.358374	1316.970952	14.211904
17.712959	1327.473800	14.216922
18.378086	1319.059981	14.221939
18.103772	1327.737601	14.226957
18.499636	1327.342848	14.231975
18.565905	1319.651124	14.236992
18.308588	1327.780743	14.242010
18.255495	1326.886450	14.247027
18.033458	1327.667265	14.252045
18.276807	1329.582407	14.257063
18.544296	1344.857084	14.262080
18.793646	1358.261237	14.267098
18.790002	1351.842082	14.272115
18.401668	1360.497820	14.277133
18.551955	1354.729699	14.282151
18.585215	1349.349565	14.287168
18.447366	1348.446248	14.292186
18.843140	1347.392358	14.297203
18.705113	1356.650137	14.302221
18.673422	1358.267084	14.307239
18.872688	1341.784614	14.312256
18.568000	1361.861024	14.317274
18.722825	1347.462155	14.322291
18.364959	1347.286234	14.327309
18.527026	1341.218776	14.332327
18.512912	1351.300435	14.337344
18.722769	1363.121398	14.342362
18.743003	1364.874822	14.347379
18.860829	1385.475643	14.352397
18.787498	1386.369072	14.357415
19.535012	1390.174236	14.362432
18.967467	1378.089465	14.367450
19.054593	1366.395656	14.372467
18.949366	1371.902129	14.377485
19.061842	1383.859064	14.382503
19.316957	1387.891442	14.387520
18.781157	1374.930690	14.392538
19.271651	1380.647338	14.397555
18.884094	1379.190098	14.402573
19.134039	1382.440375	14.407591
19.293024	1386.148138	14.412608
19.245584	1388.173733	14.417626
19.264353	1379.544300	14.422643
19.242088	1395.115888	14.427661
19.160097	1382.008102	14.432679
19.359336	1373.383687	14.437696
19.224344	1379.320018	14.442714
19.327661	1369.417554	14.447731
19.167020	1371.777752	14.452749
18.993034	1373.778201	14.457767
19.513692	1383.087556	14.462784
19.132999	1392.129197	14.467802
19.580298	1383.365570	14.472819
19.688632	1409.415805	14.477837
19.574527	1385.937291	14.482855
19.565728	1361.323470	14.487872
18.973070	1368.143770	14.492890
19.487052	1372.254607	14.497907
19.884067	1380.491250	14.502925
19.494560	1371.297888	14.507943
19.252986	1360.836965	14.512960
19.454165	1359.165131	14.517978
19.781650	1372.561502	14.522995
19.361817	1362.412474	14.528013
19.196297	1373.760517	14.533031
19.240124	1380.608890	14.538048
19.052690	1391.337432	14.543066
19.516792	1387.745654	14.548083
19.298457	1387.382329	14.553101
19.718759	1398.784348	14.558119
19.259570	1390.513772	14.563136
19.325331	1390.771511	14.568154
19.520427	1402.782908	14.573171
19.874986	1415.679837	14.578189
19.363882	1421.456322	14.583207
19.831567	1424.561784	14.588224
19.956002	1423.504113	14.593242
20.071660	1422.185726	14.598259
19.968546	1416.034126	14.603277
19.798833	1420.173522	14.608295
19.866099	1424.213530	14.613312
19.839456	1412.596549	14.618330
19.995365	1414.584213	14.623347
19.928993	1423.598730	14.628365
19.600983	1425.884443	14.633383
20.204233	1416.310495	14.638400
19.637820	1423.725017	14.643418
19.950805	1412.984058	14.648435
20.150696	1419.327792	14.653453
20.009840	1423.298271	14.658471
19.999778	1417.190733	14.663488
19.940195	1421.500879	14.668506
20.012761	1420.860578	14.673523
19.737938	1415.307742	14.678541
19.999228	1428.652315	14.683559
20.358968	1423.171950	14.688576
20.062805	1422.830736	14.693594
19.866403	1425.289554	14.698611
20.297787	1416.232519	14.703629
19.794024	1423.009614	14.708647
20.021600	1416.441215	14.713664
20.191644	1435.780115	14.718682
20.278409	1442.183294	14.723699
20.444748	1447.034573	14.728717
20.156966	1458.084818	14.733735
20.256982	1447.441618	14.738752
20.016772	1454.535555	14.743770
20.275041	1456.821619	14.748787
20.630842	1445.823598	14.753805
20.182354	1458.509223	14.758823
20.734690	1451.735589	14.763840
20.474483	1451.157167	14.768858
20.472154	1451.360814	14.773875
20.493477	1453.696661	14.778893
20.098023	1455.905348	14.783911
20.447555	1455.681808	14.788928
20.179402	1458.687844	14.793946
20.314377	1455.859786	14.798963
20.595169	1458.322220	14.803981
20.406183	1458.638788	14.808999
20.498828	1448.953951	14.814016
20.285813	1466.373209	14.819034
20.829299	1476.041002	14.824051
20.719756	1482.980307	14.829069
20.372044	1483.684864	14.834087
20.914481	1481.861165	14.839104
20.698415	1481.247498	14.844122
20.716649	1484.436693	14.849139
20.855184	1484.032893	14.854157
20.666002	1487.038678	14.859175
21.085442	1476.299569	14.864192
20.597391	1479.845813	14.869210
20.498281	1480.709260	14.874227
20.799027	1481.496591	14.879245
20.464215	1485.789254	14.884263
20.619600	1473.096823	14.889280
20.533569	1479.830892	14.894298
20.701140	1482.975529	14.899315
21.145444	1493.592660	14.904333
21.007155	1514.730199	14.909351
21.549129	1502.762528	14.914368
21.226468	1487.046962	14.919386
21.086251	1488.771805	14.924403
21.151178	1478.167449	14.929421
21.148489	1485.936417	14.934439
20.968557	1466.310634	14.939456
20.747842	1480.718818	14.944474
20.884352	1498.858589	14.949491
21.340794	1500.818055	14.954509
21.157548	1504.879800	14.959527
21.332029	1510.796729	14.964544
21.507775	1508.735437	14.969562
21.588128	1502.519237	14.974579
21.639723	1483.878058	14.979597
21.161820	1479.225564	14.984615
21.554502	1479.197424	14.989632
21.682254	1473.594968	14.994650
21.294918	1475.783224	14.999667
21.677119	1475.841646	15.004685
21.637341	1484.923053	15.009703
21.392762	1471.193331	15.014720
21.447584	1469.997772	15.019738
21.321861	1487.093618	15.024755
21.700396	1477.869124	15.029773
21.403882	1480.129368	15.034791
21.558117	1479.550755	15.039808
21.714267	1467.455164	15.044826
21.379715	1475.659819	15.049843
21.270082	1471.567445	15.054861
21.362224	1473.813454	15.059879
21.243685	1475.396544	15.064896
21.663695	1499.851946	15.069914
21.624474	1508.888400	15.074931
21.811198	1501.521514	15.079949
21.753651	1524.923355	15.084967
22.023838	1513.783157	15.089984
22.003581	1513.070408	15.095002
21.731602	1506.714623	15.100019
22.001917	1499.208155	15.105037
21.372889	1507.995273	15.110055
21.492903	1508.215115	15.115072
21.910032	1513.104488	15.120090
21.628545	1512.379797	15.125107
21.750253	1510.032398	15.130125
22.084124	1508.495489	15.135143
21.824363	1513.299896	15.140160
22.063651	1509.890299	15.145178
21.782643	1527.583227	15.150195
21.554623	1512.216118	15.155213
21.533513	1519.337254	15.160231
21.641120	1515.541009	15.165248
21.800116	1529.286968	15.170266
21.892388	1539.950103	15.175283
21.905764	1546.830350	15.180301
21.883596	1549.811894	15.185319
21.814448	1541.651757	15.190336
22.033267	1549.632347	15.195354
21.842869	1552.882800	15.200371
22.220269	1543.304567	15.205389
22.054840	1550.842230	15.210407
21.888437	1542.623962	15.215424
22.435437	1561.014432	15.220442
22.226007	1571.085604	15.225459
22.610131	1563.127286	15.230477
22.499135	1579.285298	15.235495
22.510345	1556.422541	15.240512
22.508058	1548.585165	15.245530
21.909199	1545.960236	15.250547
22.458012	1549.478439	15.255565
22.551440	1567.485075	15.260583
22.345907	1578.829253	15.265600
22.405444	1569.373797	15.270618
22.452594	1579.962931	15.275635
22.402485	1575.182635	15.280653
22.690207	1569.224817	15.285671
22.458073	1572.213704	15.290688
22.852141	1564.664316	15.295706
22.734633	1577.927343	15.300723
22.689001	1564.130218	15.305741
22.377893	1567.761006	15.310759
22.538043	1574.654604	15.315776
22.334178	1564.964567	15.320794
22.357722	1574.945083	15.325811
22.461628	1574.044907	15.330829
22.513347	1571.328408	15.335847
22.536882	1575.420362	15.340864
22.491324	1581.294556	15.345882
22.521563	1591.500915	15.350899
22.811337	1599.664268	15.355917
22.938794	1600.253698	15.360935
22.843231	1613.290128	15.365952
23.002910	1596.647021	15.370970
22.904018	1598.934065	15.375987
23.191978	1595.807115	15.381005
22.907506	1604.068908	15.386023
23.066451	1618.372163	15.391040
23.128568	1591.926026	15.396058
23.223882	1604.203051	15.401075
23.462797	1600.882854	15.406093
23.244027	1596.384523	15.411111
23.199190	1612.812308	15.416128
23.425780	1594.503250	15.421146
23.064346	1600.834911	15.426163
23.454573	1594.481849	15.431181
23.731546	1593.324560	15.436199
23.299074	1585.559434	15.441216
23.471732	1566.642672	15.446234
23.093538	1570.448697	15.451251
23.002898	1562.624536	15.456269
23.102730	1583.213636	15.461287
22.993279	1585.863595	15.466304
23.079631	1593.374236	15.471322
23.045294	1606.016932	15.476339
23.070365	1591.188945	15.481357
23.037452	1591.145910	15.486375
23.257609	1597.579860	15.491392
23.944772	1603.992537	15.496410
23.619739	1601.914198	15.501427
23.601957	1597.452525	15.506445
23.316742	1593.118304	15.511463
23.099234	1607.926809	15.516480
23.421236	1607.146082	15.521498
23.693022	1622.943484	15.526515
23.807434	1612.188554	15.531533
23.923184	1617.913879	15.536551
23.849343	1619.576200	15.541568
23.795816	1600.190543	15.546586
23.661690	1600.820642	15.551603
23.862660	1603.141784	15.556621
23.849895	1594.746545	15.561639
23.546678	1605.403829	15.566656
23.842092	1601.833383	15.571674
24.098928	1616.510566	15.576691
23.647009	1623.531115	15.581709
24.035370	1611.550954	15.586727
24.004787	1611.008783	15.591744
24.009185	1614.900196	15.596762
23.911730	1616.923261	15.601779
24.120778	1612.110166	15.606797
24.094610	1612.216784	15.611815
23.919153	1600.804150	15.616832
23.942031	1603.178734	15.621850
24.164590	1613.472208	15.626867
24.192726	1617.134140	15.631885
24.391345	1619.828458	15.636903
23.765680	1609.945138	15.641920
24.192963	1615.732942	15.646938
23.927888	1620.447721	15.651955
23.999818	1625.240651	15.656973
24.210153	1627.252613	15.661991
24.165049	1614.729792	15.667008
24.374493	1620.645316	15.672026
24.330099	1628.903271	15.677043
24.461375	1624.665154	15.682061
24.642326	1628.124103	15.687079
24.348675	1626.199805	15.692096
24.701498	1622.916875	15.697114
24.347233	1636.410390	15.702131
24.075404	1622.322683	15.707149
24.420900	1618.174348	15.712167
24.249790	1621.234251	15.717184
24.213097	1619.738098	15.722202
24.550572	1621.202741	15.727219
24.340083	1618.515195	15.732237
24.445222	1625.479709	15.737255
24.687619	1629.011761	15.742272
24.308370	1617.979005	15.747290
24.511675	1637.344547	15.752307
24.296635	1649.050536	15.757325
24.536503	1646.681818	15.762343
24.597486	1657.530693	15.767360
24.721397	1647.222339	15.772378
24.580578	1652.088028	15.777395
24.631555	1658.155327	15.782413
24.917106	1644.164050	15.787431
24.535048	1641.375342	15.792448
24.792570	1651.505210	15.797466
24.876008	1648.913950	15.802483
24.608649	1657.247343	15.807501
24.701964	1644.475867	15.812519
25.083431	1678.682114	15.817536
24.668350	1666.099737	15.822554
24.954339	1685.746913	15.827571
25.191210	1683.931961	15.832589
25.130107	1676.344365	15.837607
25.171269	1681.487628	15.842624
25.286614	1681.605305	15.847642
25.395602	1684.655347	15.852659
25.224316	1681.916436	15.857677
25.429078	1671.635645	15.862695
24.825478	1664.689796	15.867712
25.237287	1657.869816	15.872730
25.031009	1668.583163	15.877747
25.122688	1683.340057	15.882765
25.446491	1671.859431	15.887783
25.454370	1683.876595	15.892800
25.333374	1688.542195	15.897818
25.361756	1680.503055	15.902835
24.886422	1681.994555	15.907853
25.510094	1670.861176	15.912871
25.336236	1677.444315	15.917888
25.205759	1682.753129	15.922906
25.558921	1671.461328	15.927923
25.138006	1675.853300	15.932941
25.515285	1671.415090	15.937959
25.159791	1669.857258	15.942976
25.526818	1667.871212	15.947994
25.259063	1673.453069	15.953011
25.364688	1692.127040	15.958029
25.791743	1695.074923	15.963047
25.642593	1707.616613	15.968064
26.068068	1695.408629	15.973082
26.330771	1700.404673	15.978099
25.855632	1699.363004	15.983117
26.127260	1677.592911	15.988135
25.930058	1673.595455	15.993152
26.080957	1662.920867	15.998170
25.622335	1669.401276	16.003187
25.679402	1676.770950	16.008205
25.782498	1667.529270	16.013223
25.714584	1678.397492	16.018240
25.861298	1693.207891	16.023258
26.231803	1692.974191	16.028275
25.602665	1708.764477	16.033293
25.953694	1703.418704	16.038311
25.850416	1707.562157	16.043328
25.717772	1701.954820	16.048346
25.922103	1698.708419	16.053363
25.599488	1703.332548	16.058381
25.749290	1695.435322	16.063399
25.807203	1719.711768	16.068416
25.929256	1734.874270	16.073434
26.369139	1734.342724	16.078451
26.274991	1732.151025	16.083469
26.342199	1732.930512	16.088487
26.650402	1744.930571	16.093504
26.365547	1729.992072	16.098522
26.607696	1729.435137	16.103539
26.211771	1739.036709	16.108557
26.316345	1730.267917	16.113575
26.304067	1732.780401	16.118592
26.589758	1731.983230	16.123610
27.019358	1725.495278	16.128627
26.661322	1738.473822	16.133645
26.973064	1722.457534	16.138663
26.554412	1734.583800	16.143680
27.002306	1737.710705	16.148698
26.895031	1706.427424	16.153715
26.701678	1700.426629	16.158733
26.856765	1692.820226	16.163751
26.744621	1694.601468	16.168768
26.560358	1687.271984	16.173786
26.605549	1693.332774	16.178803
26.647200	1700.608169	16.183821
26.973699	1699.086828	16.188839
26.894366	1713.376208	16.193856
26.675994	1709.066534	16.198874
27.102573	1713.855997	16.203891
26.963433	1714.739258	16.208909
27.182361	1710.439789	16.213927
26.872434	1703.174365	16.218944
26.605856	1697.556096	16.223962
26.502226	1700.797359	16.228979
26.576629	1728.487979	16.233997
27.023818	1721.993185	16.239015
26.938760	1732.193890	16.244032
26.929029	1737.867957	16.249050
27.441487	1722.943753	16.254067
26.764834	1735.576572	16.259085
27.105985	1731.797972	16.264103
27.088461	1731.091454	16.269120
27.038021	1727.927891	16.274138
27.035284	1722.686629	16.279155
26.616704	1750.019636	16.284173
27.137907	1752.157387	16.289191
27.093512	1757.066616	16.294208
26.995350	1758.084036	16.299226
27.104784	1753.119072	16.304243
27.017046	1760.360569	16.309261
26.978511	1758.941665	16.314279
27.379846	1775.817089	16.319296
27.726852	1778.167072	16.324314
27.803993	1778.097387	16.329331
27.585786	1780.236872	16.334349
27.617311	1774.296905	16.339367
27.816654	1790.578243	16.344384
27.699676	1786.120705	16.349402
27.951055	1775.252291	16.354419
27.836508	1774.929672	16.359437
27.756511	1749.221031	16.364455
27.864175	1752.841706	16.369472
27.669356	1752.570340	16.374490
28.072021	1747.170553	16.379507
27.811471	1754.115054	16.384525
27.976005	1746.237609	16.389543
28.121258	1751.457974	16.394560
27.784357	1754.587815	16.399578
27.900954	1737.972736	16.404595
27.925234	1752.423551	16.409613
28.064730	1755.040075	16.414631
27.925355	1750.852947	16.419648
27.470882	1759.814288	16.424666
28.246691	1766.276945	16.429683
28.086665	1782.690289	16.434701
28.247344	1778.739165	16.439719
28.209791	1777.588174	16.444736
28.180170	1782.605587	16.449754
28.499287	1777.596124	16.454771
28.419787	1777.777886	16.459789
28.253812	1771.934329	16.464807
28.573375	1771.831866	16.469824
28.068179	1784.412772	16.474842
28.472003	1770.557329	16.479859
28.387623	1786.747770	16.484877
28.248781	1784.466020	16.489895
28.409972	1773.357622	16.494912
28.238737	1773.887376	16.499930
28.271190	1762.713262	16.504947
28.415290	1770.159729	16.509965
28.360755	1764.266267	16.514983
28.577397	1775.557161	16.520000
28.404272	1780.387289	16.525018
28.773546	1768.304663	16.530035
28.714562	1771.703897	16.535053
28.536069	1780.677708	16.540071
28.389051	1771.957750	16.545088
28.426908	1772.537587	16.550106
28.445573	1779.701872	16.555123
28.808466	1803.134842	16.560141
28.849401	1793.786050	16.565159
29.054446	1802.227654	16.570176
29.063545	1801.548815	16.575194
29.079112	1788.197620	16.580211
29.175321	1784.766337	16.585229
28.901620	1773.342647	16.590247
29.186455	1769.700889	16.595264
28.853949	1766.964591	16.600282
28.809555	1762.936545	16.605299
28.875330	1778.812437	16.610317
29.097473	1786.715839	16.615335
29.345390	1796.252385	16.620352
29.042827	1795.693151	16.625370
29.247054	1797.396734	16.630387
29.567540	1797.973564	16.635405
29.179207	1786.648128	16.640423
29.479166	1780.513031	16.645440
29.159456	1775.938819	16.650458
29.237903	1787.454108	16.655475
29.379137	1791.745344	16.660493
29.324222	1798.711782	16.665511
29.430065	1796.000668	16.670528
29.150074	1803.998669	16.675546
29.509028	1799.577623	16.680563
29.449855	1800.390792	16.685581
29.471442	1804.723060	16.690599
29.888578	1794.954073	16.695616
29.639465	1802.913708	16.700634
29.508856	1793.420253	16.705651
29.301339	1797.548086	16.710669
29.038043	1801.630616	16.715687
29.664132	1799.142547	16.720704
29.365083	1792.618696	16.725722
29.475661	1795.017396	16.730739
29.542346	1792.604449	16.735757
29.304242	1813.081021	16.740775
30.082775	1827.393881	16.745792
30.080999	1825.962008	16.750810
29.940119	1820.862228	16.755827
30.239159	1831.758096	16.760845
30.084842	1831.061778	16.765863
30.260189	1819.727412	16.770880
30.068451	1824.196303	16.775898
30.281840	1796.544643	16.780915
30.181699	1782.528996	16.785933
30.289258	1792.215096	16.790951
30.130212	1787.515917	16.795968
29.884923	1789.203635	16.800986
30.098633	1786.591809	16.806003
30.195847	1789.615474	16.811021
30.182266	1814.206603	16.816039
30.391899	1817.453006	16.821056
30.520032	1828.195247	16.826074
30.169734	1812.526626	16.831091
30.488864	1815.001089	16.836109
30.582065	1811.022529	16.841127
30.720231	1804.648640	16.846144
30.354010	1794.916200	16.851162
30.298199	1788.242524	16.856179
30.259199	1799.813643	16.861197
30.154671	1812.866485	16.866215
30.476049	1818.316398	16.871232
30.193900	1826.230920	16.876250
30.401982	1820.341475	16.881267
30.729275	1821.616308	16.886285
30.249629	1839.668560	16.891303
30.484656	1819.756850	16.896320
30.586455	1834.023299	16.901338
30.486992	1817.224967	16.906355
30.476043	1823.787349	16.911373
30.741237	1840.334989	16.916391
30.906972	1844.362379	16.921408
30.646579	1855.210964	16.926426
30.568764	1855.390677	16.931443
30.677204	1849.702310	16.936461
30.592429	1858.353629	16.941479
30.685504	1842.760905	16.946496
30.787629	1846.160891	16.951514
30.874423	1866.409455	16.956531
30.835385	1869.103134	16.961549
30.927954	1878.048742	16.966567
31.195599	1877.481685	16.971584
31.076303	1875.895429	16.976602
31.539711	1882.656188	16.981619
31.801759	1872.064848	16.986637
31.371006	1880.969392	16.991655
31.460976	1871.995280	16.996672
31.753563	1868.419926	17.001690
31.487358	1854.727289	17.006707
31.653935	1836.898081	17.011725
31.395047	1841.474716	17.016743
31.148160	1835.368554	17.021760
31.275097	1835.159750	17.026778
31.348142	1854.382544	17.031795
31.891363	1858.122978	17.036813
31.573074	1861.440687	17.041831
31.726218	1868.590466	17.046848
31.810538	1860.041063	17.051866
31.728661	1860.151574	17.056883
31.925700	1869.720980	17.061901
32.027897	1855.942467	17.066919
32.206816	1842.069801	17.071936
31.561065	1841.676122	17.076954
31.636172	1835.118373	17.081971
31.892863	1841.418648	17.086989
31.672332	1838.615610	17.092007
31.863597	1851.347787	17.097024
31.947780	1868.371971	17.102042
31.820206	1866.723705	17.107059
31.883737	1866.377167	17.112077
31.931416	1871.062581	17.117095
32.043684	1866.277407	17.122112
32.019428	1870.824528	17.127130
31.858407	1866.882650	17.132147
32.260192	1861.873277	17.137165
31.836742	1869.124046	17.142183
32.028623	1865.127984	17.147200
32.078938	1861.990455	17.152218
32.058738	1868.529585	17.157235
32.224742	1878.693032	17.162253
32.073156	1886.939708	17.167271
31.916490	1891.397115	17.172288
32.345928	1901.608176	17.177306
32.376643	1898.332162	17.182323
32.557045	1903.113159	17.187341
32.451093	1908.908689	17.192359
32.549101	1902.276270	17.197376
32.509534	1905.770935	17.202394
32.312850	1904.009494	17.207411
32.530435	1896.488322	17.212429
32.493116	1902.638804	17.217447
32.488061	1900.749448	17.222464
32.744932	1913.639516	17.227482
32.679996	1932.277994	17.232499
33.033109	1921.083056	17.237517
33.004678	1928.764189	17.242535
33.007514	1917.312015	17.247552
32.880568	1902.904080	17.252570
32.616725	1898.232813	17.257587
32.901549	1907.381484	17.262605
33.153800	1927.909642	17.267623
33.061757	1931.458058	17.272640
32.944272	1928.720447	17.277658
32.898233	1924.310391	17.282675
33.147107	1929.852828	17.287693
33.110387	1929.191987	17.292711
33.060359	1923.487856	17.297728
33.323892	1921.178565	17.302746
32.910359	1928.078550	17.307763
33.175481	1917.778174	17.312781
32.949746	1924.133403	17.317799
33.040739	1929.086842	17.322816
33.227794	1923.629917	17.327834
33.054063	1930.168462	17.332851
33.223217	1934.282899	17.337869
33.145801	1960.182694	17.342887
33.544145	1947.787285	17.347904
33.777878	1954.094549	17.352922
33.481184	1947.501943	17.357939
33.804294	1946.508640	17.362957
33.815166	1954.629894	17.367975
33.669545	1947.615321	17.372992
34.283707	1938.812983	17.378010
33.937337	1948.611984	17.383027
34.202697	1938.113151	17.388045
34.002021	1921.016702	17.393063
33.530024	1920.129007	17.398080
33.807876	1915.430418	17.403098
33.645930	1923.258204	17.408115
34.156859	1927.274040	17.413133
33.993928	1936.911633	17.418151
34.041963	1952.546765	17.423168
34.297606	1941.293715	17.428186
33.814519	1941.731127	17.433203
34.022196	1939.971948	17.438221
34.310797	1949.622915	17.443239
34.076885	1950.815125	17.448256
34.320770	1941.421881	17.453274
34.211203	1951.735233	17.458291
34.359501	1939.427996	17.463309
34.347959	1943.697282	17.468327
34.348691	1949.154761	17.473344
34.576406	1945.276169	17.478362
34.402327	1950.904449	17.483379
34.454177	1945.921187	17.488397
34.337009	1941.106785	17.493415
34.574701	1946.681585	17.498432
34.554513	1942.671734	17.503450
34.218717	1945.861660	17.508467
34.175467	1942.331157	17.513485
34.289932	1933.420473	17.518503
34.271742	1940.105938	17.523520
34.325717	1945.623704	17.528538
34.693927	1965.168882	17.533555
34.380434	1968.710402	17.538573
34.678342	1971.439353	17.543591
34.901639	1978.882085	17.548608
34.886009	1972.752416	17.553626
34.799638	1976.001906	17.558643
34.813863	1974.896670	17.563661
34.867698	1966.267412	17.568679
34.369974	1978.667536	17.573696
34.877004	1963.704435	17.578714
34.843086	1974.274169	17.583731
35.069978	1979.462029	17.588749
35.170189	1982.097091	17.593767
35.184872	1993.220556	17.598784
35.501716	1996.460107	17.603802
35.209125	1986.358921	17.608819
35.524744	1980.604974	17.613837
35.309607	1967.707253	17.618855
35.229152	1968.693810	17.623872
35.566014	1954.047586	17.628890
35.315835	1973.183602	17.633907
35.387293	1970.880457	17.638925
35.553830	1972.104121	17.643943
35.430466	1985.610959	17.648960
35.468186	1996.612326	17.653978
35.505316	1999.573529	17.658995
35.549738	2002.814206	17.664013
35.610115	1997.197106	17.669031
35.433583	2000.635891	17.674048
35.710368	1993.411549	17.679066
35.767464	2010.156538	17.684083
35.830445	2003.627097	17.689101
35.992561	1997.987280	17.694119
35.731962	1997.967500	17.699136
36.072196	1995.764408	17.704154
35.869966	2004.953272	17.709171
35.760773	1999.700968	17.714189
36.109946	1986.347617	17.719207
36.054825	2002.078577	17.724224
36.193628	1998.257179	17.729242
36.187903	1994.988741	17.734259
35.596494	1998.555133	17.739277
35.926982	1983.834942	17.744295
35.515880	1995.976304	17.749312
36.022829	2005.871313	17.754330
35.828372	2009.504774	17.759347
36.267761	2016.780333	17.764365
36.194057	2019.822250	17.769383
36.073244	2032.175091	17.774400
36.463785	2026.666593	17.779418
36.344248	2023.844273	17.784435
36.416954	2036.244854	17.789453
36.514207	2017.514785	17.794471
36.393999	2030.867024	17.799488
36.631282	2031.960118	17.804506
36.892225	2040.764426	17.809523
36.668329	2046.399399	17.814541
36.929201	2038.717084	17.819559
36.560262	2043.454272	17.824576
36.758385	2035.912826	17.829594
36.898396	2042.865862	17.834611
36.823015	2048.606988	17.839629
36.955370	2045.301354	17.844647
36.966451	2046.406437	17.849664
37.039408	2037.366149	17.854682
37.225603	2030.985412	17.859699
37.305997	2042.267524	17.864717
37.203111	2033.840683	17.869735
36.930939	2034.599505	17.874752
37.170605	2041.019198	17.879770
37.293633	2040.676800	17.884787
37.421860	2040.753970	17.889805
37.292798	2042.310710	17.894823
37.253834	2036.113225	17.899840
37.291845	2039.973997	17.904858
37.157007	2034.485983	17.909875
37.463257	2035.752307	17.914893
37.322512	2028.045822	17.919911
37.019651	2039.404059	17.924928
37.500983	2035.467000	17.929946
37.460181	2036.683205	17.934963
37.394571	2042.298712	17.939981
37.421728	2031.012889	17.944999
37.116288	2041.650961	17.950016
37.434709	2030.859075	17.955034
37.692374	2050.694254	17.960051
37.763627	2057.160483	17.965069
37.940344	2064.661342	17.970087
37.684865	2065.656358	17.975104
37.693239	2056.183471	17.980122
37.725004	2070.305822	17.985139
37.637704	2076.554781	17.990157
37.698592	2066.654552	17.995175
37.786395	2074.371663	18.000192
37.937680	2058.499641	18.005210
37.754287	2073.447625	18.010227
37.840829	2073.661001	18.015245
38.309233	2074.476757	18.020263
38.163006	2073.319690	18.025280
38.074987	2088.477101	18.030298
38.107228	2081.613371	18.035315
38.481680	2083.416206	18.040333
38.630104	2087.676615	18.045351
38.233964	2093.733728	18.050368
38.249974	2094.072134	18.055386
38.698173	2081.944336	18.060403
38.526366	2093.536638	18.065421
38.922098	2087.510581	18.070439
38.994460	2092.456326	18.075456
38.903274	2076.830435	18.080474
38.401529	2058.926980	18.085491
38.477933	2067.640946	18.090509
38.720673	2073.872369	18.095527
38.931996	2085.584405	18.100544
38.812265	2080.660355	18.105562
39.033705	2082.148943	18.110579
39.088047	2082.487707	18.115597
39.065588	2081.278891	18.120615
38.735673	2085.118395	18.125632
38.893714	2078.318713	18.130650
38.976447	2074.570137	18.135667
38.840137	2082.000304	18.140685
38.716772	2082.742411	18.145703
38.955923	2083.723204	18.150720
38.752619	2074.747835	18.155738
38.837237	2082.024971	18.160755
38.738874	2103.441334	18.165773
39.177170	2102.650420	18.170791
38.999062	2109.907605	18.175808
39.182774	2117.025679	18.180826
39.406504	2114.566261	18.185843
38.905480	2122.054156	18.190861
39.278568	2109.972209	18.195879
39.479830	2115.069675	18.200896
39.386117	2131.992655	18.205914
39.943074	2129.319523	18.210931
39.814023	2137.078995	18.215949
39.853199	2129.122869	18.220967
39.664512	2123.049883	18.225984
39.650013	2130.362907	18.231002
39.851734	2125.352065	18.236019
39.559497	2134.966665	18.241037
39.926763	2129.952676	18.246055
39.815860	2133.988852	18.251072
39.762920	2135.404688	18.256090
40.020189	2129.678634	18.261107
40.120423	2132.123973	18.266125
40.095601	2127.474944	18.271143
40.017615	2131.577720	18.276160
39.989940	2130.135730	18.281178
40.425011	2135.670699	18.286195
40.598414	2131.126890	18.291213
40.594293	2127.980981	18.296231
40.532835	2137.356089	18.301248
40.650217	2124.031869	18.306266
40.632307	2123.430307	18.311283
40.281560	2118.780419	18.316301
40.513867	2116.731550	18.321319
40.349416	2121.643806	18.326336
40.499206	2132.772209	18.331354
40.741261	2133.983407	18.336371
40.505732	2143.037319	18.341389
40.111391	2135.191800	18.346407
40.202055	2132.034361	18.351424
40.220382	2128.703068	18.356442
40.704396	2126.937176	18.361459
40.063102	2134.421685	18.366477
40.649924	2142.985802	18.371495
40.945888	2162.240246	18.376512
40.518585	2169.073526	18.381530
40.855640	2158.778226	18.386547
41.038274	2162.903685	18.391565
41.138508	2159.128184	18.396583
41.155040	2158.994899	18.401600
40.962262	2165.340843	18.406618
41.382220	2147.826851	18.411635
41.042449	2160.530907	18.416653
41.350831	2154.589134	18.421671
41.460009	2148.111243	18.426688
41.129485	2155.738483	18.431706
41.083814	2151.565877	18.436723
41.102391	2164.289254	18.441741
41.415806	2172.581080	18.446759
41.735504	2186.672097	18.451776
41.507682	2180.376642	18.456794
41.877284	2178.051360	18.461811
41.861162	2192.132135	18.466829
41.637432	2187.773806	18.471847
41.610708	2176.433007	18.476864
41.024504	2176.391843	18.481882
41.581901	2175.453108	18.486899
41.384549	2185.856902	18.491917
41.851657	2183.863899	18.496935
42.009744	2180.827973	18.501952
41.475842	2182.434107	18.506970
42.150396	2190.509981	18.511987
42.020238	2215.421772	18.517005
42.037613	2203.958716	18.522023
42.440847	2210.032583	18.527040
42.346134	2210.279851	18.532058
42.574020	2201.530174	18.537075
41.926205	2195.428316	18.542093
42.169137	2192.761204	18.547111
42.898832	2200.584097	18.552128
42.743115	2193.696067	18.557146
42.490910	2176.793855	18.562163
42.515258	2181.572186	18.567181
42.343456	2181.505058	18.572199
42.325088	2163.407639	18.577216
42.013615	2183.332511	18.582234
42.623857	2184.504326	18.587251
42.604674	2199.871119	18.592269
42.633227	2205.777592	18.597287
42.834067	2201.787836	18.602304
42.367259	2206.882355	18.607322
42.831150	2206.417097	18.612339
42.917535	2211.657976	18.617357
43.014162	2211.912597	18.622375
43.268475	2203.013881	18.627392
43.081352	2206.691053	18.632410
42.862527	2203.834325	18.637427
43.162407	2204.396271	18.642445
43.155767	2205.067525	18.647463
42.798064	2207.279917	18.652480
42.678327	2208.742031	18.657498
43.019221	2210.826188	18.662515
43.067794	2209.216094	18.667533
43.382179	2223.383804	18.672551
43.488059	2236.105017	18.677568
43.582943	2242.032626	18.682586
43.783606	2220.760655	18.687603
43.245931	2200.631490	18.692621
43.278454	2222.382655	18.697639
43.722989	2225.559820	18.702656
43.588573	2236.018399	18.707674
43.737308	2231.357980	18.712691
43.601059	2228.797021	18.717709
43.740169	2242.708502	18.722727
43.647424	2232.951063	18.727744
43.804601	2232.412879	18.732762
43.405235	2235.998371	18.737779
43.530927	2227.158884	18.742797
43.610714	2241.759238	18.747815
44.116084	2229.032956	18.752832
43.494229	2237.679940	18.757850
43.904265	2259.462072	18.762867
43.831054	2258.880469	18.767885
43.752469	2264.526938	18.772903
44.096752	2253.340699	18.777920
43.957668	2260.978871	18.782938
44.206462	2265.072167	18.787955
44.427780	2255.586998	18.792973
44.289225	2272.795470	18.797991
44.716887	2278.723215	18.803008
44.753718	2275.439419	18.808026
44.823499	2263.237410	18.813043
44.810987	2257.167933	18.818061
44.854035	2253.718759	18.823079
44.573215	2251.128345	18.828096
44.471541	2254.579420	18.833114
44.505928	2244.945637	18.838131
44.840373	2258.241640	18.843149
44.674918	2284.134482	18.848167
45.337340	2275.668830	18.853184
45.130307	2278.554697	18.858202
45.452709	2277.230221	18.863219
45.367224	2259.025484	18.868237
44.930771	2244.921303	18.873255
45.170487	2241.230204	18.878272
45.194372	2236.499280	18.883290
45.003231	2238.442443	18.888307
45.012392	2247.084756	18.893325
44.714469	2262.429372	18.898343
45.241106	2270.140200	18.903360
45.148650	2268.240440	18.908378
45.003012	2270.491217	18.913395
45.039143	2270.978847	18.918413
45.224062	2276.756368	18.923431
45.459920	2264.550141	18.928448
45.444836	2283.918336	18.933466
45.418186	2301.185308	18.938483
45.452771	2305.931084	18.943501
45.596551	2310.216139	18.948519
45.614205	2298.490588	18.953536
45.642515	2309.234504	18.958554
45.749876	2299.291214	18.963571
46.060004	2296.939329	18.968589
45.722585	2309.097103	18.973607
45.777126	2302.753363	18.978624
45.580621	2307.080476	18.983642
45.841269	2292.257764	18.988659
45.936120	2312.597111	18.993677
45.868006	2330.938196	18.998695
46.091083	2320.387436	19.003712
46.088368	2336.971025	19.008730
46.000852	2330.937534	19.013747
46.211892	2335.274271	19.018765
46.220739	2325.244890	19.023783
46.305398	2320.338559	19.028800
46.297512	2330.237168	19.033818
46.881481	2333.901703	19.038835
46.694973	2316.377117	19.043853
46.477521	2329.303596	19.048871
46.655091	2331.697411	19.053888
46.797424	2351.421142	19.058906
46.611803	2356.646787	19.063923
47.144803	2353.129224	19.068941
46.772426	2364.319083	19.073959
47.005908	2348.375706	19.078976
47.124045	2362.314972	19.083994
47.333083	2352.295205	19.089011
47.285021	2338.019877	19.094029
47.110090	2331.516424	19.099047
47.265243	2312.986647	19.104064
46.978167	2317.474780	19.109082
47.230960	2338.810806	19.114099
47.431213	2339.708485	19.119117
47.136154	2353.579223	19.124135
47.351524	2347.367733	19.129152
47.302216	2350.457253	19.134170
47.323547	2356.617317	19.139187
47.578876	2355.921583	19.144205
47.383367	2357.938114	19.149223
47.602035	2351.198760	19.154240
47.295681	2354.738399	19.159258
47.406328	2348.273764	19.164275
47.336285	2342.729661	19.169293
47.360437	2353.391625	19.174311
47.585746	2359.726233	19.179328
47.677694	2370.424640	19.184346
47.675092	2377.901548	19.189363
48.233910	2381.385227	19.194381
47.946772	2386.444208	19.199399
47.928130	2377.056684	19.204416
47.933563	2378.103872	19.209434
47.947545	2379.123664	19.214451
48.155008	2380.744502	19.219469
47.791068	2385.211501	19.224487
48.252147	2394.293741	19.229504
48.373237	2408.229411	19.234522
48.244032	2400.096459	19.239539
48.476333	2407.008231	19.244557
48.245054	2413.118139	19.249575
48.252390	2402.187260	19.254592
48.781715	2406.798954	19.259610
48.572217	2410.222806	19.264627
48.996066	2401.042242	19.269645
48.679243	2406.558066	19.274663
49.042541	2401.998546	19.279680
48.935263	2393.831858	19.284698
48.657764	2402.953284	19.289715
48.940318	2392.604834	19.294733
49.178340	2398.189585	19.299751
48.994594	2396.422995	19.304768
49.139361	2396.185650	19.309786
48.817733	2399.566026	19.314803
48.955676	2391.477115	19.319821
48.774894	2406.761378	19.324839
49.133352	2396.611388	19.329856
49.224945	2406.573128	19.334874
49.207471	2419.190871	19.339891
49.727881	2406.199382	19.344909
49.420824	2416.064813	19.349927
49.829813	2425.253113	19.354944
49.940244	2411.618795	19.359962
49.449760	2406.920459	19.364979
49.649011	2392.426078	19.369997
49.578657	2398.521199	19.375015
49.722674	2421.121667	19.380032
49.667647	2414.526323	19.385050
49.435318	2416.478480	19.390067
49.638601	2408.481510	19.395085
49.502094	2420.027478	19.400103
49.808544	2411.449724	19.405120
49.873189	2411.820058	19.410138
49.759080	2423.256431	19.415155
49.966080	2422.392710	19.420173
50.175821	2441.789104	19.425191
50.337367	2447.245577	19.430208
50.006852	2440.792391	19.435226
50.295641	2453.391244	19.440243
50.608694	2443.428830	19.445261
50.218004	2450.120956	19.450279
50.580026	2447.181583	19.455296
50.779733	2437.902614	19.460314
50.137297	2453.601766	19.465331
50.637019	2443.716568	19.470349
50.653294	2453.389234	19.475367
50.522503	2443.029139	19.480384
50.563116	2438.165085	19.485402
50.181272	2454.112884	19.490419
51.025974	2457.992218	19.495437
50.755397	2472.098761	19.500455
50.880316	2477.363479	19.505472
50.982392	2473.037640	19.510490
50.907789	2473.762259	19.515507
51.287767	2474.894990	19.520525
51.166748	2477.014769	19.525543
51.228806	2473.645469	19.530560
51.233768	2469.662032	19.535578
51.016398	2480.222076	19.540595
51.373592	2464.335493	19.545613
51.543412	2471.617235	19.550631
51.284653	2458.721389	19.555648
51.452938	2475.510119	19.560666
51.497810	2502.010252	19.565683
51.903137	2497.926399	19.570701
51.867515	2512.670874	19.575719
51.638295	2504.642773	19.580736
51.839503	2493.249904	19.585754
51.849050	2503.063662	19.590771
51.906786	2490.605413	19.595789
52.084524	2496.902865	19.600807
51.986825	2506.770368	19.605824
52.071496	2494.511193	19.610842
52.050648	2496.443569	19.615859
52.206763	2500.397531	19.620877
52.227868	2492.539275	19.625895
52.086947	2494.813712	19.630912
52.435658	2494.975505	19.635930
52.160966	2499.835434	19.640947
52.246501	2495.201913	19.645965
52.185496	2495.268824	19.650983
52.049579	2496.983423	19.656000
52.320804	2487.212328	19.661018
52.282337	2497.330647	19.666035
52.291925	2500.859250	19.671053
52.597249	2500.857754	19.676071
52.733290	2518.472268	19.681088
52.709933	2526.920520	19.686106
52.389937	2520.797624	19.691123
52.311726	2515.020574	19.696141
52.482910	2511.461986	19.701159
52.706695	2536.232348	19.706176
52.822386	2546.544697	19.711194
52.769756	2544.612734	19.716211
53.138204	2549.179408	19.721229
52.938645	2550.939368	19.726247
53.154557	2550.300923	19.731264
53.330653	2533.875141	19.736282
53.047530	2552.145924	19.741299
53.463320	2552.000986	19.746317
53.442229	2560.525056	19.751335
53.649594	2577.464908	19.756352
54.110792	2564.531494	19.761370
53.937161	2562.747663	19.766387
53.923847	2551.669905	19.771405
53.894410	2542.042743	19.776423
54.199679	2533.990670	19.781440
54.206675	2524.531698	19.786458
53.806157	2538.923338	19.791475
53.581012	2522.801649	19.796493
53.945437	2518.307258	19.801511
53.462092	2543.464934	19.806528
54.061151	2549.513861	19.811546
54.317326	2548.508159	19.816563
54.059486	2562.138502	19.821581
54.249206	2562.411011	19.826599
54.249786	2567.779765	19.831616
54.371054	2563.740472	19.836634
54.163436	2570.528767	19.841651
54.216131	2562.837290	19.846669
54.318540	2565.351429	19.851687
54.452294	2585.795328	19.856704
54.686540	2585.465444	19.861722
54.746647	2601.649594	19.866739
54.964722	2599.810479	19.871757
54.946945	2593.260475	19.876775
54.874169	2607.171081	19.881792
55.075608	2592.082689	19.886810
55.142846	2602.569016	19.891827
55.155262	2588.089579	19.896845
55.116699	2589.577091	19.901863
55.091538	2596.927528	19.906880
55.152143	2591.931981	19.911898
55.366396	2585.034015	19.916915
55.333571	2595.379600	19.921933
55.510326	2589.128530	19.926951
55.450170	2593.333199	19.931968
55.327751	2584.166030	19.936986
55.548199	2600.116020	19.942003
55.678040	2592.342494	19.947021
55.367716	2594.055807	19.952039
55.334746	2587.865967	19.957056
55.660755	2598.019984	19.962074
55.219747	2592.533548	19.967091
55.322640	2603.249991	19.972109
55.087623	2616.446128	19.977127
55.032258	2630.464107	19.982144
55.645508	2624.276515	19.987162
55.625379	2657.033883	19.992179
55.747072	2652.510671	19.997197
56.225114	2649.967415	20.002215
55.730096	2654.664601	20.007232
55.936049	2653.482164	20.012250
56.237714	2656.162591	20.017267
56.104882	2660.216700	20.022285
56.738517	2662.403520	20.027303
56.557341	2676.834627	20.032320
56.800679	2675.021052	20.037338
56.715653	2682.757578	20.042355
56.711909	2684.624360	20.047373
56.822942	2671.520979	20.052391
56.915078	2676.996287	20.057408
56.878295	2674.827058	20.062426
56.982349	2669.904616	20.067443
56.571296	2676.630714	20.072461
56.750959	2678.104219	20.077479
56.906520	2679.712014	20.082496
57.227568	2675.207818	20.087514
56.964740	2667.825498	20.092531
56.901884	2671.172226	20.097549
57.262294	2676.441401	20.102567
56.861878	2672.156222	20.107584
57.279552	2681.299542	20.112602
57.551333	2701.495604	20.117619
57.276380	2698.440984	20.122637
57.781866	2703.630097	20.127655
57.588106	2710.797634	20.132672
57.732170	2703.817322	20.137690
57.500113	2706.617840	20.142707
57.508124	2700.089906	20.147725
57.693435	2699.867706	20.152743
57.896395	2704.500943	20.157760
57.967371	2699.910119	20.162778
58.350391	2700.925640	20.167795
58.351465	2712.887056	20.172813
58.414018	2701.590170	20.177831
57.981201	2700.117049	20.182848
58.118990	2698.655143	20.187866
58.534835	2710.254729	20.192883
58.011328	2716.299274	20.197901
58.673836	2728.364775	20.202919
58.207513	2729.625760	20.207936
57.990285	2727.830415	20.212954
58.473103	2730.666341	20.217971
58.372627	2719.843599	20.222989
58.657995	2715.786992	20.228007
58.739478	2723.999930	20.233024
58.747901	2728.655873	20.238042
58.821626	2735.219019	20.243059
58.666950	2752.422026	20.248077
59.211599	2746.152618	20.253095
58.918644	2751.380385	20.258112
58.941313	2748.173430	20.263130
59.110960	2747.113318	20.268147
59.287331	2744.801776	20.273165
59.528317	2749.748015	20.278183
59.366786	2741.432047	20.283200
59.317933	2736.805898	20.288218
59.506732	2740.557682	20.293235
59.700812	2754.021395	20.298253
59.656854	2738.627370	20.303271
59.623854	2745.726629	20.308288
59.447420	2745.310283	20.313306
59.644089	2751.180720	20.318323
59.501439	2745.533122	20.323341
59.916124	2734.798853	20.328359
59.799112	2751.901941	20.333376
60.035331	2764.390647	20.338394
60.053621	2776.596891	20.343411
59.886986	2779.364566	20.348429
60.116441	2765.081172	20.353447
60.029673	2782.156855	20.358464
60.265168	2774.679540	20.363482
60.153258	2769.849247	20.368499
60.200752	2772.914195	20.373517
60.294113	2765.843813	20.378535
59.992792	2779.276032	20.383552
60.022125	2784.963909	20.388570
60.559624	2792.565339	20.393587
60.535415	2817.301939	20.398605
60.892183	2809.590013	20.403623
60.973793	2794.953090	20.408640
61.176382	2806.377765	20.413658
61.065894	2798.913518	20.418675
60.814500	2794.782606	20.423693
61.159769	2808.323739	20.428711
60.714638	2799.966419	20.433728
61.061173	2795.312709	20.438746
61.419181	2794.021479	20.443763
61.240238	2806.180421	20.448781
60.894884	2802.709878	20.453799
61.506010	2824.984158	20.458816
61.352572	2818.606467	20.463834
61.413284	2819.196150	20.468851
61.528008	2824.280987	20.473869
61.880650	2808.621760	20.478887
61.839078	2828.389481	20.483904
61.903192	2812.655100	20.488922
61.808001	2810.735647	20.493939
61.830943	2832.809118	20.498957
61.965365	2812.676746	20.503975
61.917336	2812.545856	20.508992
62.041104	2817.491803	20.514010
61.909367	2821.796546	20.519027
62.090535	2839.827963	20.524045
62.202462	2852.182170	20.529063
62.146449	2848.032342	20.534080
62.150542	2852.067024	20.539098
62.590974	2843.183838	20.544115
62.202235	2847.678293	20.549133
62.307126	2847.555596	20.554151
62.501554	2856.825473	20.559168
62.803092	2875.993279	20.564186
62.775319	2887.618669	20.569203
62.652765	2883.433374	20.574221
62.924916	2887.923744	20.579239
63.278164	2883.957446	20.584256
62.839994	2874.139955	20.589274
63.343910	2885.403484	20.594291
62.810506	2884.398911	20.599309
63.059531	2871.267244	20.604327
63.211124	2883.524769	20.609344
62.945383	2878.308071	20.614362
63.337378	2875.635306	20.619379
63.578648	2891.809310	20.624397
63.374325	2894.226165	20.629415
63.267362	2908.067694	20.634432
63.382468	2912.096645	20.639450
63.703713	2901.087952	20.644467
63.536076	2910.474775	20.649485
63.685027	2909.343272	20.654503
63.579068	2908.418451	20.659520
63.456047	2919.142721	20.664538
63.829861	2926.944486	20.669555
63.804549	2938.032132	20.674573
64.037454	2935.763580	20.679591
64.081248	2935.497836	20.684608
63.966494	2931.782082	20.689626
64.361957	2929.283923	20.694643
64.301008	2943.939887	20.699661
64.161305	2935.258414	20.704679
64.516321	2938.032038	20.709696
64.135675	2941.107928	20.714714
64.717553	2949.309554	20.719731
64.680609	2951.849933	20.724749
64.809169	2959.433592	20.729767
65.119911	2959.555212	20.734784
64.982125	2966.477408	20.739802
64.883064	2953.823644	20.744819
65.029527	2956.143175	20.749837
65.210407	2961.690332	20.754855
65.228625	2950.547828	20.759872
65.191257	2956.125930	20.764890
65.314510	2950.844929	20.769907
64.940528	2960.736329	20.774925
65.092707	2950.405903	20.779943
65.261620	2959.403299	20.784960
65.058799	2981.563104	20.789978
65.865662	2984.001848	20.794995
65.853244	2984.648895	20.800013
65.880553	2976.649217	20.805031
65.933153	2979.000402	20.810048
66.034440	2977.001220	20.815066
66.144741	2972.994735	20.820083
66.140716	2981.032183	20.825101
66.075041	2972.687259	20.830119
65.948262	2978.252586	20.835136
65.836186	2982.124616	20.840154
66.261850	2968.823133	20.845171
66.128243	2979.945633	20.850189
66.011713	2985.459665	20.855207
66.629513	3000.363744	20.860224
66.457498	3010.315498	20.865242
66.503088	2998.712945	20.870259
66.410158	3013.471894	20.875277
66.673439	3010.825099	20.880295
66.419530	3004.108044	20.885312
66.273280	3025.290496	20.890330
66.717530	3024.841653	20.895347
66.780234	3038.534401	20.900365
67.023954	3041.269352	20.905383
66.851742	3036.359179	20.910400
66.742453	3042.870812	20.915418
67.104757	3032.375693	20.920435
67.177110	3054.908618	20.925453
67.014194	3066.393095	20.930471
67.408837	3064.030872	20.935488
67.111981	3061.103809	20.940506
67.609175	3066.295204	20.945523
67.650139	3064.574078	20.950541
67.435115	3059.899310	20.955559
67.751554	3061.928575	20.960576
67.747137	3069.283878	20.965594
68.097440	3079.529667	20.970611
68.284609	3091.351179	20.975629
68.097031	3073.973542	20.980647
68.594077	3063.275042	20.985664
68.408891	3065.573411	20.990682
68.539864	3051.950096	20.995699
68.313757	3058.639693	21.000717
68.418423	3053.118038	21.005735
68.502213	3050.821750	21.010752
68.436799	3056.443103	21.015770
68.604595	3056.286389	21.020787
68.468228	3066.640934	21.025805
68.619167	3089.312886	21.030823
68.812867	3085.176060	21.035840
68.628483	3094.396083	21.040858
68.862658	3080.319485	21.045875
68.873233	3086.343631	21.050893
68.660005	3090.753249	21.055911
68.693522	3077.337347	21.060928
68.772116	3101.584203	21.065946
68.935361	3106.409157	21.070963
69.181958	3114.045825	21.075981
69.189894	3117.525237	21.080999
69.483008	3110.058319	21.086016
69.432922	3113.679202	21.091034
69.605086	3124.778443	21.096051
69.826339	3113.207011	21.101069
69.435563	3116.134220	21.106087
69.768122	3126.937676	21.111104
69.846409	3135.214350	21.116122
69.980437	3143.933771	21.121139
69.864886	3149.397700	21.126157
69.884431	3146.459281	21.131175
69.965796	3140.177692	21.136192
69.989490	3141.964801	21.141210
70.216197	3144.312437	21.146227
69.938942	3157.958321	21.151245
70.562133	3170.461362	21.156263
70.588905	3176.521447	21.161280
70.591969	3172.062568	21.166298
70.839576	3172.268636	21.171315
70.781613	3173.779882	21.176333
70.837164	3167.512783	21.181351
71.067997	3159.621501	21.186368
70.857360	3176.698797	21.191386
71.254194	3161.615358	21.196403
71.180175	3156.812933	21.201421
71.049524	3172.867200	21.206439
71.109375	3170.618549	21.211456
71.138743	3169.711899	21.216474
71.329520	3164.422817	21.221491
71.601014	3163.226954	21.226509
71.547755	3163.355578	21.231527
71.740809	3160.043220	21.236544
71.626255	3178.357748	21.241562
71.856900	3191.018976	21.246579
71.924953	3190.068139	21.251597
71.891386	3196.905895	21.256615
71.881995	3198.870519	21.261632
71.764127	3198.427160	21.266650
71.787484	3200.565896	21.271667
71.822666	3194.680487	21.276685
71.923122	3193.945941	21.281703
72.175822	3194.257071	21.286720
72.129092	3206.196847	21.291738
72.244439	3220.562138	21.296755
72.374381	3223.507255	21.301773
72.230091	3231.499510	21.306791
72.284286	3231.436761	21.311808
72.095735	3232.602279	21.316826
72.360085	3239.359723	21.321843
72.623724	3250.706924	21.326861
72.704873	3254.011674	21.331879
73.172980	3242.495415	21.336896
73.070064	3244.132202	21.341914
72.907069	3253.335399	21.346931
73.520002	3241.341285	21.351949
73.485316	3238.862584	21.356967
73.672472	3237.627110	21.361984
73.506964	3232.122871	21.367002
73.372513	3221.216811	21.372019
73.620041	3237.027162	21.377037
74.168722	3234.933939	21.382055
73.696587	3226.425341	21.387072
73.770721	3233.974823	21.392090
73.710641	3229.118499	21.397107
73.842494	3218.955027	21.402125
73.500368	3232.737283	21.407143
73.849663	3246.283254	21.412160
73.898408	3255.117221	21.417178
73.955644	3261.938820	21.422195
74.201277	3265.939996	21.427213
74.284777	3266.960170	21.432231
74.192774	3265.626339	21.437248
74.664267	3275.638459	21.442266
74.507339	3286.816605	21.447283
74.661096	3291.982153	21.452301
74.835748	3297.884389	21.457319
74.647040	3286.197111	21.462336
74.397521	3280.789806	21.467354
74.794617	3292.771660	21.472371
74.986749	3283.678867	21.477389
74.542017	3295.406926	21.482407
75.057197	3303.222924	21.487424
74.762259	3313.009362	21.492442
74.513472	3323.090929	21.497459
74.964034	3323.642982	21.502477
75.375558	3333.076086	21.507495
75.206274	3348.611733	21.512512
75.547793	3346.177540	21.517530
75.410259	3347.120861	21.522547
75.824003	3341.860228	21.527565
75.708768	3336.306307	21.532583
75.832563	3334.524615	21.537600
76.113151	3369.831574	21.542618
76.120774	3384.797877	21.547635
76.437379	3377.184826	21.552653
76.421286	3369.513765	21.557671
76.272041	3374.795550	21.562688
76.336942	3370.642531	21.567706
76.228797	3376.369090	21.572723
76.582688	3363.170862	21.577741
76.474540	3369.062377	21.582759
76.390071	3373.866144	21.587776
76.418042	3360.237138	21.592794
76.523895	3383.405544	21.597811
76.722784	3397.434366	21.602829
76.761697	3398.984349	21.607847
76.880112	3401.684165	21.612864
76.963750	3400.422084	21.617882
77.032549	3409.992969	21.622899
77.554940	3418.865295	21.627917
77.292775	3425.111410	21.632935
77.338921	3428.149939	21.637952
77.839107	3434.757477	21.642970
77.622476	3436.009145	21.647987
77.898612	3436.732542	21.653005
77.434134	3430.648905	21.658023
78.073366	3425.911605	21.663040
77.755611	3423.342644	21.668058
77.773477	3433.162506	21.673075
77.870066	3430.791214	21.678093
77.772022	3435.735037	21.683111
77.734578	3428.814706	21.688128
78.341387	3449.905583	21.693146
78.233540	3457.093912	21.698163
78.235771	3459.322786	21.703181
78.194493	3464.756050	21.708199
78.290834	3456.536847	21.713216
78.694837	3449.927807	21.718234
78.977930	3460.540856	21.723251
78.808995	3446.815180	21.728269
78.635764	3453.325345	21.733287
79.062022	3464.865120	21.738304
79.235538	3472.974272	21.743322
78.843531	3479.807998	21.748339
79.454958	3478.266180	21.753357
79.574694	3481.361456	21.758375
79.334697	3479.072152	21.763392
79.576480	3469.608453	21.768410
79.441654	3479.529559	21.773427
79.323083	3480.463849	21.778445
79.494940	3476.723831	21.783463
79.147990	3486.466217	21.788480
79.673969	3488.953428	21.793498
79.573676	3497.941686	21.798515
79.561039	3512.962641	21.803533
80.038015	3513.891436	21.808551
79.809893	3504.300248	21.813568
80.356816	3528.840065	21.818586
80.265617	3533.625309	21.823603
80.236487	3526.715372	21.828621
80.673636	3533.410928	21.833639
80.366991	3530.119647	21.838656
80.264433	3529.611150	21.843674
80.428652	3533.934901	21.848691
81.344060	3530.340112	21.853709
81.131433	3545.625640	21.858727
81.041095	3531.869184	21.863744
81.236203	3530.886702	21.868762
81.081183	3538.206877	21.873779
81.164271	3535.867327	21.878797
81.193923	3551.769119	21.883815
81.540188	3561.632829	21.888832
81.700913	3552.738374	21.893850
81.429095	3564.344362	21.898867
81.745164	3560.270260	21.903885
81.790117	3562.565712	21.908903
81.507789	3563.443208	21.913920
81.840569	3553.521118	21.918938
81.989151	3554.727800	21.923955
81.960687	3557.342072	21.928973
81.750194	3555.667955	21.933991
81.867186	3572.659264	21.939008
82.207854	3576.002696	21.944026
81.549444	3587.797385	21.949043
82.020017	3589.020548	21.954061
82.030041	3602.743759	21.959079
82.350473	3607.862186	21.964096
82.740842	3617.296992	21.969114
82.430517	3618.457856	21.974131
82.599034	3614.515996	21.979149
82.804886	3624.070271	21.984167
83.041840	3633.899728	21.989184
83.548283	3641.268524	21.994202
83.322723	3633.692181	21.999219
83.236873	3617.762474	22.004237
83.387864	3624.895905	22.009255
83.204977	3642.038417	22.014272
83.333029	3640.039452	22.019290
83.135821	3642.174143	22.024307
83.232616	3642.846872	22.029325
83.503629	3635.865243	22.034343
83.537514	3647.429045	22.039360
83.646737	3650.817824	22.044378
83.619586	3664.529516	22.049395
83.638533	3665.210778	22.054413
84.084427	3662.660078	22.059431
84.070528	3668.421959	22.064448
84.214198	3653.452319	22.069466
84.004541	3676.842195	22.074483
84.463659	3690.005054	22.079501
84.411740	3686.660625	22.084519
84.405431	3700.712212	22.089536
84.638575	3689.028151	22.094554
84.805673	3696.177063	22.099571
84.742367	3697.956171	22.104589
84.979090	3690.584908	22.109607
84.799321	3713.693917	22.114624
84.953918	3713.929931	22.119642
85.202817	3726.255115	22.124659
85.365197	3713.900837	22.129677
85.503887	3714.937906	22.134695
85.372316	3722.154293	22.139712
85.603125	3721.829681	22.144730
85.707819	3723.943631	22.149747
85.705432	3724.072514	22.154765
85.581668	3718.024982	22.159783
85.556426	3744.325044	22.164800
85.551535	3741.545275	22.169818
85.621279	3739.795697	22.174835
85.677626	3750.843659	22.179853
85.977841	3765.856076	22.184871
85.857417	3775.494674	22.189888
86.432171	3777.527808	22.194906
86.114224	3785.438411	22.199923
86.372977	3782.995781	22.204941
86.790539	3798.325062	22.209959
86.881760	3805.051914	22.214976
87.182792	3795.687282	22.219994
87.180314	3804.573333	22.225011
87.365925	3803.148306	22.230029
87.335689	3793.443923	22.235047
87.083792	3799.751089	22.240064
87.261336	3798.736846	22.245082
87.227874	3797.910228	22.250099
87.749032	3801.995544	22.255117
87.714171	3795.945890	22.260135
87.299663	3793.750730	22.265152
87.829425	3791.661351	22.270170
87.883993	3796.468258	22.275187
87.654315	3794.324447	22.280205
87.997557	3813.256994	22.285223
87.909693	3825.750504	22.290240
88.020348	3825.537871	22.295258
88.240844	3822.330289	22.300275
88.242307	3819.179768	22.305293
88.420413	3814.922490	22.310311
88.485621	3821.324511	22.315328
88.886008	3812.729286	22.320346
88.544939	3821.511845	22.325363
88.828044	3851.444635	22.330381
88.931376	3845.729217	22.335399
88.697788	3846.954584	22.340416
88.793030	3851.420925	22.345434
89.062283	3851.110037	22.350451
88.957851	3842.898609	22.355469
89.326909	3843.628326	22.360487
88.884701	3851.315793	22.365504
89.324611	3851.308992	22.370522
89.614669	3866.557834	22.375539
89.305828	3875.028008	22.380557
89.833307	3880.078060	22.385575
89.441765	3869.571117	22.390592
89.585584	3864.916338	22.395610
89.361492	3876.651681	22.400627
89.959735	3891.313001	22.405645
90.217093	3895.938790	22.410663
90.192207	3909.729459	22.415680
90.182237	3910.813941	22.420698
90.323651	3903.102023	22.425715
90.098704	3903.681075	22.430733
90.502014	3909.495367	22.435751
90.331544	3929.679495	22.440768
90.751684	3932.499628	22.445786
91.017817	3930.215207	22.450803
91.019602	3930.408364	22.455821
91.219808	3924.113121	22.460839
90.714994	3939.985907	22.465856
91.006703	3925.764786	22.470874
91.274375	3959.456298	22.475891
91.069773	3962.085176	22.480909
91.203639	3957.350910	22.485927
90.961229	3960.926210	22.490944
91.502025	3974.376214	22.495962
92.212130	3972.783006	22.500979
92.089257	3985.328492	22.505997
92.069527	3982.368058	22.511015
92.174755	3979.846827	22.516032
92.408147	3978.334753	22.521050
92.815335	3983.071640	22.526067
92.455583	3991.420365	22.531085
92.659540	3974.497110	22.536103
92.653233	3975.299490	22.541120
92.578467	3974.168264	22.546138
92.872057	3980.563322	22.551155
92.710976	3973.590736	22.556173
93.028051	3971.056549	22.561191
92.943325	3977.196002	22.566208
92.628457	3972.763443	22.571226
92.815618	3996.131930	22.576243
92.663441	4011.898093	22.581261
93.300865	4001.687579	22.586279
93.058680	4005.714042	22.591296
93.300160	4020.360025	22.596314
93.398322	4046.263821	22.601331
93.258399	4042.984251	22.606349
93.776553	4035.526951	22.611367
93.481101	4046.363563	22.616384
93.800864	4059.231252	22.621402
93.783634	4069.241179	22.626419
93.971748	4074.568638	22.631437
94.777496	4066.296853	22.636455
94.469413	4072.646878	22.641472
94.569360	4072.704128	22.646490
94.881236	4067.519144	22.651507
94.901595	4065.585165	22.656525
95.052808	4057.874701	22.661543
94.934178	4065.263916	22.666560
94.974581	4055.944557	22.671578
95.154579	4064.952183	22.676595
95.001911	4088.322236	22.681613
95.162222	4080.553563	22.686631
95.612902	4083.883258	22.691648
95.328808	4083.412220	22.696666
95.761630	4088.422077	22.701683
95.422947	4088.941974	22.706701
95.647762	4078.724784	22.711719
95.680993	4090.327215	22.716736
95.638466	4074.823356	22.721754
95.819294	4067.570210	22.726771
95.933072	4090.404888	22.731789
95.788879	4092.314732	22.736807
95.796828	4110.300657	22.741824
95.713858	4113.459084	22.746842
96.433059	4122.689465	22.751859
96.381797	4145.956231	22.756877
96.604005	4143.204615	22.761895
96.661549	4142.708620	22.766912
96.519752	4147.689819	22.771930
96.680436	4138.719839	22.776947
96.748531	4145.062065	22.781965
96.958551	4159.498805	22.786983
97.024224	4169.192332	22.792000
97.360745	4175.992989	22.797018
97.193265	4170.249363	22.802035
97.319076	4187.940304	22.807053
97.496169	4172.144538	22.812071
97.564285	4180.210846	22.817088
97.392343	4199.263640	22.822106
97.645214	4198.735367	22.827123
97.762361	4207.050288	22.832141
97.883284	4200.545980	22.837159
97.782674	4206.966898	22.842176
98.208066	4229.948327	22.847194
98.426029	4225.491433	22.852211
98.365497	4225.135422	22.857229
98.539074	4241.960627	22.862247
98.651212	4231.371392	22.867264
98.641247	4243.461405	22.872282
98.994793	4243.943698	22.877299
98.971820	4258.664708	22.882317
98.976097	4252.207607	22.887335
99.538974	4258.577969	22.892352
99.041603	4243.982989	22.897370
99.518082	4248.622679	22.902387
99.158315	4260.645306	22.907405
99.391824	4253.863307	22.912423
99.561851	4275.272374	22.917440
99.316097	4277.350604	22.922458
99.808769	4296.082270	22.927475
99.723644	4288.615477	22.932493
99.921750	4282.484617	22.937511
99.845861	4302.363036	22.942528
99.908782	4309.204629	22.947546
100.764982	4310.564141	22.952563
100.694100	4313.758801	22.957581
100.586253	4314.062996	22.962599
101.256659	4312.182998	22.967616
100.769490	4313.247537	22.972634
100.863156	4315.325200	22.977651
100.955754	4316.146295	22.982669
101.116255	4303.788318	22.987687
101.349959	4322.892743	22.992704
101.112744	4338.844554	22.997722
101.385732	4344.874254	23.002739
101.405152	4350.430479	23.007757
101.524308	4349.001423	23.012775
101.395098	4336.342064	23.017792
101.298754	4350.181546	23.022810
101.537910	4344.106479	23.027827
101.824344	4374.296824	23.032845
101.508969	4367.573975	23.037863
102.007508	4375.670054	23.042880
101.772306	4370.055660	23.047898
102.081452	4384.030934	23.052915
102.108533	4400.485224	23.057933
102.162264	4404.970790	23.062951
102.068000	4398.579913	23.067968
101.846537	4419.713301	23.072986
102.657633	4424.306021	23.078003
102.612848	4436.799594	23.083021
102.983931	4440.411038	23.088039
103.174218	4439.429691	23.093056
103.101022	4455.545867	23.098074
103.434252	4461.445574	23.103091
103.148624	4459.606204	23.108109
103.498224	4467.996639	23.113127
104.070784	4459.398990	23.118144
103.612413	4462.628574	23.123162
103.799803	4470.665086	23.128179
103.926348	4478.314786	23.133197
104.092027	4487.962851	23.138215
104.566591	4499.037519	23.143232
104.367654	4493.538354	23.148250
104.544909	4486.126935	23.153267
104.407674	4487.858503	23.158285
104.544711	4483.442862	23.163303
104.709169	4481.374385	23.168320
104.932389	4490.831833	23.173338
104.844768	4508.372174	23.178355
105.117543	4524.789147	23.183373
104.804076	4522.508283	23.188391
105.208757	4522.149414	23.193408
104.997865	4524.706980	23.198426
105.323595	4512.447133	23.203443
105.019881	4524.597715	23.208461
105.231314	4533.878386	23.213479
105.693992	4537.747174	23.218496
105.466844	4542.588263	23.223514
105.773770	4558.181867	23.228531
105.907446	4571.948102	23.233549
106.085609	4574.017743	23.238567
106.747984	4560.556103	23.243584
105.878971	4569.992491	23.248602
106.282109	4576.285437	23.253619
106.510986	4589.305994	23.258637
106.597396	4592.805054	23.263655
106.868148	4587.231396	23.268672
106.732543	4593.992526	23.273690
106.858159	4595.391286	23.278707
107.400367	4608.217556	23.283725
107.057628	4627.615255	23.288743
107.627363	4624.593125	23.293760
107.625086	4623.598308	23.298778
107.596091	4620.466044	23.303795
108.255083	4611.341795	23.308813
107.586689	4615.286075	23.313831
107.952806	4612.392874	23.318848
107.505534	4615.389537	23.323866
108.069667	4626.603443	23.328883
107.989529	4632.803422	23.333901
108.473350	4641.839925	23.338919
108.500655	4640.237819	23.343936
108.018874	4641.726711	23.348954
108.616149	4644.709059	23.353971
108.065624	4653.305813	23.358989
108.210271	4676.949687	23.364007
108.958079	4670.533343	23.369024
108.948174	4676.945765	23.374042
109.116075	4673.018703	23.379059
109.096215	4684.618142	23.384077
109.229635	4700.054719	23.389095
109.598270	4705.642744	23.394112
109.300731	4702.200483	23.399130
109.554059	4705.636158	23.404147
109.564259	4699.782264	23.409165
109.448727	4721.777354	23.414183
109.916963	4732.086647	23.419200
109.842197	4740.043381	23.424218
110.207499	4733.921728	23.429235
110.130443	4735.451240	23.434253
110.071964	4748.417830	23.439271
110.823076	4749.619148	23.444288
110.793179	4753.918618	23.449306
111.125449	4752.995687	23.454323
110.910961	4753.328535	23.459341
111.121231	4754.965307	23.464359
111.439113	4749.345612	23.469376
111.235218	4763.477660	23.474394
111.300013	4748.331014	23.479411
111.457203	4762.074239	23.484429
111.419288	4769.902056	23.489447
111.633877	4773.774099	23.494464
112.140551	4782.680127	23.499482
112.323862	4775.043933	23.504499
112.164901	4773.289508	23.509517
111.935257	4781.260436	23.514535
112.331247	4764.725096	23.519552
112.098411	4783.277605	23.524570
112.303307	4790.186114	23.529587
112.436357	4799.483046	23.534605
112.430497	4806.948866	23.539623
112.873204	4798.804804	23.544640
112.600621	4812.293474	23.549658
112.701204	4830.397610	23.554675
113.691459	4840.725452	23.559693
113.030618	4848.198329	23.564711
113.169183	4840.200572	23.569728
113.204324	4830.877683	23.574746
113.249574	4842.792490	23.579763
113.611930	4853.437888	23.584781
113.627993	4865.678031	23.589799
113.963081	4863.207661	23.594816
114.270714	4862.590392	23.599834
114.296169	4863.632470	23.604851
114.396934	4874.121092	23.609869
114.121690	4890.040375	23.614887
114.172271	4902.178773	23.619904
114.476356	4894.008352	23.624922
114.541368	4891.623945	23.629939
114.819702	4908.582966	23.634957
114.373656	4926.773993	23.639975
115.207216	4927.271097	23.644992
115.062522	4929.435869	23.650010
115.040786	4921.848841	23.655027
115.441714	4944.771585	23.660045
115.386034	4956.688588	23.665063
115.708935	4962.473648	23.670080
115.750971	4958.985457	23.675098
115.707625	4962.750549	23.680115
115.690789	4959.869772	23.685133
115.907917	4966.129041	23.690151
115.890786	4978.540913	23.695168
115.940444	4981.861867	23.700186
116.296802	4984.204506	23.705203
116.660591	4996.839302	23.710221
116.402269	5013.613467	23.715239
116.593284	5015.861769	23.720256
116.952608	5016.426213	23.725274
116.744145	5005.703585	23.730291
117.438203	5004.959463	23.735309
117.001257	5017.653351	23.740327
117.141130	5018.692676	23.745344
117.250927	5035.931281	23.750362
117.333939	5042.830118	23.755379
117.510759	5029.394369	23.760397
117.377107	5038.769373	23.765415
117.707070	5054.451802	23.770432
118.054173	5071.620916	23.775450
117.735926	5068.564313	23.780467
118.138171	5066.356854	23.785485
118.081784	5086.687026	23.790503
118.381999	5095.723421	23.795520
118.463115	5092.726031	23.800538
118.636157	5104.330919	23.805555
118.626066	5094.582631	23.810573
118.654593	5120.344191	23.815591
119.238488	5131.205164	23.820608
118.973271	5129.048138	23.825626
118.964203	5131.477562	23.830643
119.280365	5141.098017	23.835661
119.273430	5158.493460	23.840679
119.614160	5152.917882	23.845696
119.346939	5156.670796	23.850714
119.805261	5184.437231	23.855731
120.001260	5179.459630	23.860749
119.787135	5191.515995	23.865767
120.167177	5191.191110	23.870784
120.118350	5196.712846	23.875802
120.203590	5222.267545	23.880819
120.654422	5219.723659	23.885837
120.283221	5226.495248	23.890855
120.676216	5249.006717	23.895872
120.734550	5258.819862	23.900890
120.994660	5257.752906	23.905907
121.205670	5252.061706	23.910925
121.274263	5271.872204	23.915943
121.770011	5262.895827	23.920960
121.697055	5283.904257	23.925978
121.705141	5276.147152	23.930995
121.820023	5276.745303	23.936013
121.965813	5286.705842	23.941031
122.134157	5287.075846	23.946048
122.476470	5305.930830	23.951066
122.457554	5310.191627	23.956083
122.710265	5306.769345	23.961101
122.976285	5300.742626	23.966119
122.913369	5309.730869	23.971136
122.953612	5300.183212	23.976154
122.772168	5300.072769	23.981171
123.103621	5293.718673	23.986189
122.966718	5317.433269	23.991207
123.103913	5324.612678	23.996224
123.441891	5334.393839	24.001242
123.275803	5334.801385	24.006259
123.575219	5341.231874	24.011277
123.636308	5357.089757	24.016295
123.800212	5358.123166	24.021312
123.967354	5358.403204	24.026330
123.852926	5372.167829	24.031347
124.361361	5376.545073	24.036365
124.756887	5378.954932	24.041383
124.599022	5374.563356	24.046400
124.956130	5386.493196	24.051418
124.875799	5392.175735	24.056435
125.110389	5380.616566	24.061453
124.507533	5380.461569	24.066471
124.805733	5384.906628	24.071488
125.390219	5403.205909	24.076506
125.389206	5415.939910	24.081523
125.427686	5410.340160	24.086541
125.516437	5421.003594	24.091559
125.562830	5417.782327	24.096576
125.553819	5425.871473	24.101594
125.551675	5446.703442	24.106611
125.931257	5432.726700	24.111629
126.261382	5449.626565	24.116647
126.121104	5473.023020	24.121664
126.201077	5479.585112	24.126682
126.348582	5481.684747	24.131699
126.603034	5474.516435	24.136717
126.657429	5491.258339	24.141735
126.749912	5506.164619	24.146752
127.000165	5502.167437	24.151770
126.971740	5522.589628	24.156787
127.358154	5532.589315	24.161805
127.314205	5534.867460	24.166823
127.382190	5546.984189	24.171840
127.501022	5541.763288	24.176858
127.679533	5567.924475	24.181875
127.913746	5569.713696	24.186893
128.108316	5575.375684	24.191911
127.881144	5576.693833	24.196928
128.409480	5573.766961	24.201946
128.029754	5597.578803	24.206963
128.389397	5603.604912	24.211981
128.943354	5611.825963	24.216999
128.968328	5632.120561	24.222016
129.273059	5622.690837	24.227034
129.477685	5633.233681	24.232051
129.303793	5628.852557	24.237069
129.392830	5627.750450	24.242087
129.373518	5647.776761	24.247104
129.993174	5650.329179	24.252122
129.768822	5650.404979	24.257139
129.888095	5654.416630	24.262157
130.178468	5652.535884	24.267175
130.043284	5667.570499	24.272192
130.204987	5689.828658	24.277210
130.111127	5697.967008	24.282227
130.587721	5681.652457	24.287245
130.577531	5708.928661	24.292263
130.827067	5721.671124	24.297280
131.058431	5708.466757	24.302298
131.023562	5722.049624	24.307315
131.046848	5723.350419	24.312333
131.366856	5739.150944	24.317351
131.218939	5747.136813	24.322368
131.781065	5739.004823	24.327386
131.724110	5747.577710	24.332403
132.074041	5761.306111	24.337421
131.963264	5779.588021	24.342439
131.884054	5771.274151	24.347456
132.274762	5768.239653	24.352474
132.508852	5786.508294	24.357491
132.779408	5795.822474	24.362509
133.221634	5795.831446	24.367527
133.091232	5807.290512	24.372544
133.646720	5795.654784	24.377562
133.230977	5800.904243	24.382579
133.452283	5786.182369	24.387597
133.644186	5785.197524	24.392615
133.536694	5793.233438	24.397632
133.834822	5795.577162	24.402650
133.702959	5793.442501	24.407667
133.631340	5790.867907	24.412685
134.081905	5806.982013	24.417703
133.697155	5828.650649	24.422720
133.939578	5817.534021	24.427738
134.146075	5829.080369	24.432755
134.238848	5852.973601	24.437773
134.303611	5855.288168	24.442791
134.459473	5861.978846	24.447808
134.851676	5875.684612	24.452826
135.085923	5893.402487	24.457843
134.733857	5903.381106	24.462861
135.114412	5899.934423	24.467879
135.022049	5902.447031	24.472896
135.375045	5913.937340	24.477914
135.819045	5912.545427	24.482931
136.114879	5922.682001	24.487949
136.501959	5936.972217	24.492967
136.606470	5936.537707	24.497984
136.684701	5927.227915	24.503002
136.631885	5935.594680	24.508019
136.550203	5939.644333	24.513037
136.787811	5932.156897	24.518055
136.757139	5928.364710	24.523072
137.087516	5934.378852	24.528090
136.877318	5939.655427	24.533107
137.240721	5959.650006	24.538125
137.198988	5969.263170	24.543143
137.387300	5979.793587	24.548160
137.660314	5990.345454	24.553178
137.759993	5996.433178	24.558195
137.751053	5987.172799	24.563213
138.125193	5997.926892	24.568231
138.020463	6026.199729	24.573248
138.345087	6025.128757	24.578266
138.832687	6030.010493	24.583283
138.699598	6027.013275	24.588301
138.805099	6033.382771	24.593319
138.692098	6047.843919	24.598336
138.852230	6057.011122	24.603354
139.005723	6066.658239	24.608371
138.758860	6074.161728	24.613389
139.200033	6079.621317	24.618407
139.401913	6089.873933	24.623424
139.688119	6096.246672	24.628442
139.994401	6123.291750	24.633459
139.956272	6122.654785	24.638477
140.222559	6122.651091	24.643495
140.029745	6121.538819	24.648512
140.462324	6135.075912	24.653530
140.484147	6143.383990	24.658547
140.454682	6141.434362	24.663565
140.669517	6152.813403	24.668583
140.977433	6175.630076	24.673600
141.057007	6170.035866	24.678618
141.399829	6171.734760	24.683635
141.534977	6179.486251	24.688653
141.659897	6189.482315	24.693671
141.714370	6197.174692	24.698688
142.130959	6183.378602	24.703706
142.468819	6189.885387	24.708723
142.542513	6191.285389	24.713741
142.617439	6195.928229	24.718759
142.642034	6192.374131	24.723776
143.019386	6185.825056	24.728794
142.694612	6179.971617	24.733811
142.759191	6197.737165	24.738829
142.735232	6191.915133	24.743847
142.747255	6218.903469	24.748864
142.890770	6228.507446	24.753882
142.907129	6228.489922	24.758899
142.888612	6251.621314	24.763917
143.588379	6252.769032	24.768935
143.532547	6264.104673	24.773952
143.911782	6275.621234	24.778970
144.014290	6289.881614	24.783987
143.613464	6288.457186	24.789005
144.176042	6291.836604	24.794023
144.251069	6318.198849	24.799040
144.694206	6320.387569	24.804058
144.824104	6321.408156	24.809075
144.551847	6336.880302	24.814093
144.911536	6348.637982	24.819111
144.903381	6356.547120	24.824128
145.149336	6357.505218	24.829146
145.289061	6373.014070	24.834163
145.421292	6380.400725	24.839181
145.789379	6388.536739	24.844199
145.722945	6410.666659	24.849216
146.037186	6400.764345	24.854234
146.150400	6408.545562	24.859251
146.293537	6415.372855	24.864269
146.325084	6424.755253	24.869287
146.771612	6443.207706	24.874304
146.800093	6428.497405	24.879322
146.981495	6446.480194	24.884339
146.745846	6467.151276	24.889357
147.226830	6460.380992	24.894375
147.278375	6490.872548	24.899392
147.378462	6492.839973	24.904410
147.657141	6494.195108	24.909427
147.828828	6508.698633	24.914445
148.093376	6516.297390	24.919463
148.240468	6533.260564	24.924480
148.440777	6531.220944	24.929498
148.499460	6532.378531	24.934515
148.339500	6544.059198	24.939533
148.659490	6557.384510	24.944551
148.998907	6571.451642	24.949568
148.974492	6560.410476	24.954586
148.952073	6572.688237	24.959603
149.032172	6591.531393	24.964621
149.468596	6590.656913	24.969639
149.445570	6617.426484	24.974656
149.935118	6623.237394	24.979674
149.759080	6615.050909	24.984691
149.771678	6627.599356	24.989709
150.441946	6632.453463	24.994727
150.514848	6652.781626	24.999744
150.512217	6664.775821	25.004762
150.428268	6655.803873	25.009779
150.760316	6671.142632	25.014797
151.056448	6685.658048	25.019815
150.677539	6683.888950	25.024832
151.000007	6699.374229	25.029850
151.149070	6718.625121	25.034867
151.325458	6722.179490	25.039885
151.644351	6744.520280	25.044903
151.931253	6741.249552	25.049920
151.731471	6752.910177	25.054938
151.999466	6768.706947	25.059955
151.949558	6778.887421	25.064973
152.819993	6783.351739	25.069991
152.391574	6784.265356	25.075008
152.698028	6800.069978	25.080026
152.964400	6810.984986	25.085043
152.835646	6825.510880	25.090061
152.845170	6812.701372	25.095079
153.460999	6830.124532	25.100096
153.869855	6850.920380	25.105114
154.082210	6845.648155	25.110131
153.654502	6853.463053	25.115149
154.003858	6845.142383	25.120167
154.068320	6844.252956	25.125184
154.244893	6861.422680	25.130202
154.457892	6869.385316	25.135219
154.528608	6866.524375	25.140237
154.852644	6882.519128	25.145255
154.913414	6901.114616	25.150272
154.865687	6897.291148	25.155290
155.305295	6903.111990	25.160307
155.192883	6908.204191	25.165325
155.070813	6916.433281	25.170343
155.272875	6944.321573	25.175360
155.613096	6951.283498	25.180378
155.661312	6959.042650	25.185395
155.764458	6984.324761	25.190413
156.396837	6998.883355	25.195431
156.298837	7002.894236	25.200448
156.041645	7020.579992	25.205466
156.509175	7022.101650	25.210483
156.710076	7047.759920	25.215501
156.884183	7049.669506	25.220519
157.282956	7057.494433	25.225536
157.139575	7058.573611	25.230554
157.673049	7060.294658	25.235571
157.920543	7085.454634	25.240589
158.145550	7079.860487	25.245607
158.893864	7087.863159	25.250624
158.524412	7086.906013	25.255642
159.216491	7079.364995	25.260659
158.973276	7093.591082	25.265677
158.797205	7083.044001	25.270695
159.097660	7083.207931	25.275712
159.003525	7084.873592	25.280730
159.227590	7103.062726	25.285747
158.999186	7117.999142	25.290765
159.404299	7108.083734	25.295783
159.280436	7136.587759	25.300800
159.198552	7149.070326	25.305818
159.771292	7160.444516	25.310835
159.495047	7183.679717	25.315853
159.838893	7180.532592	25.320871
160.136554	7209.839736	25.325888
160.075511	7221.081629	25.330906
160.532728	7223.235863	25.335923
160.859846	7241.604237	25.340941
160.593206	7249.485650	25.345959
160.926923	7270.950524	25.350976
161.081387	7282.511265	25.355994
161.266694	7284.383588	25.361011
161.465825	7306.984390	25.366029
161.641235	7313.954806	25.371047
162.101862	7339.369803	25.376064
161.988986	7348.031558	25.381082
162.769136	7338.321032	25.386099
162.771490	7345.475998	25.391117
162.869908	7354.936111	25.396135
163.205069	7364.160216	25.401152
163.054470	7364.989367	25.406170
163.482333	7358.939457	25.411187
163.373972	7366.507307	25.416205
163.228711	7356.376312	25.421223
163.634709	7365.413082	25.426240
163.757148	7382.388333	25.431258
163.706274	7389.556839	25.436275
163.970908	7406.324325	25.441293
164.072970	7417.290531	25.446311
164.574602	7419.068862	25.451328
164.687494	7418.256461	25.456346
164.541300	7421.672117	25.461363
164.876316	7436.070752	25.466381
165.147256	7449.195426	25.471399
165.452371	7446.626439	25.476416
165.079718	7463.272458	25.481434
165.311115	7468.769560	25.486451
165.408875	7484.817278	25.491469
165.496395	7502.169383	25.496487
165.682744	7516.840747	25.501504
165.621580	7535.768229	25.506522
166.452656	7541.054434	25.511539
166.278316	7555.656265	25.516557
166.476474	7570.960530	25.521575
166.778296	7582.645999	25.526592
166.545918	7595.925629	25.531610
166.891118	7601.605599	25.536627
167.175709	7616.566412	25.541645
166.988074	7632.789814	25.546663
167.758917	7636.576175	25.551680
168.020032	7649.585287	25.556698
168.116400	7663.273764	25.561715
168.309466	7671.766219	25.566733
168.219231	7677.893061	25.571751
168.372436	7679.556508	25.576768
168.681952	7709.929037	25.581786
169.051266	7711.654443	25.586803
169.089963	7723.783595	25.591821
169.187657	7754.465294	25.596839
169.656667	7747.572002	25.601856
169.489531	7748.379489	25.606874
169.957896	7763.222652	25.611891
169.967272	7775.068424	25.616909
169.731433	7777.297080	25.621927
170.312482	7790.827613	25.626944
170.404530	7810.425566	25.631962
170.501422	7801.446714	25.636979
170.520737	7834.001061	25.641997
170.750169	7838.974069	25.647015
171.053984	7840.466153	25.652032
171.296683	7863.341730	25.657050
171.784394	7861.815234	25.662067
171.856651	7874.513913	25.667085
171.937766	7878.901828	25.672103
172.402985	7887.025723	25.677120
172.478281	7904.062881	25.682138
172.447897	7902.218727	25.687156
172.929087	7902.114160	25.692173
172.696032	7906.665046	25.697191
172.833982	7909.411644	25.702208
172.875377	7933.422455	25.707226
173.167368	7927.767323	25.712244
173.384883	7942.177170	25.717261
173.339060	7958.615334	25.722279
173.743986	7959.414161	25.727296
173.799346	7977.914934	25.732314
174.177333	7980.729787	25.737332
174.606058	7978.046566	25.742349
174.660826	7989.940132	25.747367
174.744136	7988.450514	25.752384
174.824904	8013.485932	25.757402
174.886085	8014.226566	25.762420
175.688409	8015.081816	25.767437
175.067717	8027.622596	25.772455
175.346067	8017.249483	25.777472
175.673057	8034.101061	25.782490
175.575261	8039.861474	25.787508
176.020397	8045.374658	25.792525
176.268160	8071.608114	25.797543
176.548269	8062.885536	25.802560
176.239333	8083.235311	25.807578
176.552134	8078.952663	25.812596
176.843319	8090.017257	25.817613
176.750679	8102.496051	25.822631
177.196627	8105.984931	25.827648
177.408400	8117.766013	25.832666
177.548155	8142.854900	25.837684
177.574120	8139.786102	25.842701
177.692528	8140.689776	25.847719
177.916932	8164.153230	25.852736
178.132147	8171.519926	25.857754
178.366053	8183.782579	25.862772
178.902195	8201.045574	25.867789
178.823688	8200.412833	25.872807
179.089934	8196.571829	25.877824
178.770496	8230.113938	25.882842
179.258470	8238.601290	25.887860
179.563226	8236.455195	25.892877
179.210910	8271.904163	25.897895
179.448761	8265.096888	25.902912
180.031751	8286.598358	25.907930
180.137889	8298.908202	25.912948
180.647449	8294.178693	25.917965
180.727041	8312.378127	25.922983
181.297743	8325.356335	25.928000
180.878789	8323.954399	25.933018
181.229977	8332.264343	25.938036
181.756447	8337.369587	25.943053
181.411770	8353.571628	25.948071
181.657270	8352.267051	25.953088
181.699352	8357.995016	25.958106
181.975643	8372.796452	25.963124
182.457035	8382.966575	25.968141
181.977620	8387.253487	25.973159
182.397259	8395.333980	25.978176
182.774748	8418.095148	25.983194
182.758162	8427.439430	25.988212
182.850486	8444.555484	25.993229
183.008826	8462.730265	25.998247
183.213578	8473.983478	26.003264
183.257135	8496.480937	26.008282
183.789091	8506.856237	26.013300
183.803795	8512.547036	26.018317
183.911862	8530.563221	26.023335
184.461604	8548.807331	26.028352
184.376539	8560.023424	26.033370
184.585552	8577.757547	26.038388
184.872926	8586.952458	26.043405
184.896963	8596.228692	26.048423
185.118967	8612.804440	26.053440
185.577385	8626.978197	26.058458
185.375332	8642.338597	26.063476
185.736811	8647.368022	26.068493
185.847951	8659.292158	26.073511
186.277475	8671.095961	26.078528
186.240824	8683.533667	26.083546
186.627411	8699.229285	26.088564
186.987178	8701.906291	26.093581
186.915439	8726.147298	26.098599
186.773181	8721.971961	26.103616
187.372660	8733.221576	26.108634
187.247613	8749.279821	26.113652
187.796282	8742.018497	26.118669
187.281287	8774.161319	26.123687
187.987019	8775.816296	26.128704
188.572735	8793.552220	26.133722
188.519692	8808.788128	26.138740
188.728057	8808.188304	26.143757
188.550978	8818.921984	26.148775
188.791412	8831.536931	26.153792
189.527185	8844.377234	26.158810
189.313038	8845.956572	26.163828
189.561417	8851.326114	26.168845
189.740119	8875.232959	26.173863
189.611060	8865.907248	26.178880
189.888865	8877.796135	26.183898
189.981762	8902.992424	26.188916
190.647339	8911.846991	26.193933
190.515034	8919.576281	26.198951
191.160208	8916.068693	26.203968
191.327569	8944.065491	26.208986
191.157778	8960.521236	26.214004
191.573183	8962.595194	26.219021
191.649059	8974.615976	26.224039
191.870877	8989.891712	26.229056
191.903867	8990.555133	26.234074
192.148398	9014.218162	26.239092
192.886502	9021.472868	26.244109
192.900014	9018.750169	26.249127
193.063864	9033.225014	26.254144
193.290262	9050.987513	26.259162
193.117071	9057.420031	26.264180
193.431341	9059.423281	26.269197
193.588760	9090.508861	26.274215
193.232630	9093.366444	26.279232
193.993924	9112.126046	26.284250
194.154063	9128.710980	26.289268
194.328831	9129.519544	26.294285
194.251272	9154.589223	26.299303
194.565997	9152.392525	26.304320
194.922868	9177.849677	26.309338
194.710904	9200.065828	26.314356
195.087650	9216.330713	26.319373
195.041778	9237.466348	26.324391
195.459003	9243.027888	26.329408
195.501449	9260.027033	26.334426
195.651231	9292.307605	26.339444
196.152183	9287.754882	26.344461
196.310004	9322.869056	26.349479
196.618849	9324.636931	26.354496
196.976312	9350.480227	26.359514
197.082915	9364.659998	26.364532
197.083979	9362.273277	26.369549
197.031784	9390.274053	26.374567
197.417761	9401.503495	26.379584
197.733567	9405.344999	26.384602
198.092619	9420.960025	26.389620
198.653890	9443.847475	26.394637
198.450309	9445.849689	26.399655
198.674907	9463.794903	26.404672
198.955458	9468.192843	26.409690
199.272927	9484.051896	26.414708
199.757814	9490.281335	26.419725
199.370743	9493.843571	26.424743
199.429574	9505.983361	26.429760
199.798388	9509.368723	26.434778
199.920768	9534.782482	26.439796
200.256303	9537.645594	26.444813
200.589335	9562.986784	26.449831
200.445837	9559.874820	26.454848
201.000551	9577.058268	26.459866
200.478387	9589.339802	26.464884
200.926635	9597.905345	26.469901
200.942962	9619.984323	26.474919
200.953818	9645.083489	26.479936
201.454545	9651.757000	26.484954
201.798888	9672.102479	26.489972
202.037342	9687.907836	26.494989
202.090893	9706.451093	26.500007
202.149427	9728.305841	26.505024
202.415977	9748.336586	26.510042
202.749841	9755.656059	26.515060
203.456575	9770.106470	26.520077
203.548203	9781.747948	26.525095
203.785981	9781.012471	26.530112
203.845429	9802.601713	26.535130
204.186365	9819.652176	26.540148
204.221872	9820.339635	26.545165
204.566313	9840.546676	26.550183
204.925126	9856.066856	26.555200
205.134623	9858.895711	26.560218
205.336635	9881.689546	26.565236
205.428827	9889.282961	26.570253
205.277545	9891.089902	26.575271
205.431126	9909.484532	26.580288
206.036285	9919.737599	26.585306
205.414479	9939.384441	26.590324
205.876912	9954.748172	26.595341
206.191125	9967.894568	26.600359
206.354601	9997.970279	26.605376
206.875522	10017.512698	26.610394
207.106641	10031.026561	26.615412
207.082772	10044.056368	26.620429
207.191631	10060.577487	26.625447
207.757536	10082.241762	26.630464
207.933162	10086.563471	26.635482
208.223546	10102.760035	26.640500
208.420767	10121.319422	26.645517
208.950943	10126.371074	26.650535
209.069241	10143.446065	26.655552
209.536535	10150.821660	26.660570
209.309159	10154.516775	26.665588
209.365676	10166.335271	26.670605
209.535063	10182.349461	26.675623
209.755164	10200.903585	26.680640
210.235859	10210.017083	26.685658
210.389076	10231.047093	26.690676
210.523192	10237.734161	26.695693
210.484496	10260.610057	26.700711
210.720204	10270.373770	26.705728
210.961504	10290.670107	26.710746
211.046671	10303.322905	26.715764
211.040653	10321.567926	26.720781
211.615571	10335.028395	26.725799
212.093286	10348.185902	26.730816
212.571045	10362.238280	26.735834
212.866112	10387.323163	26.740852
213.039860	10388.110693	26.745869
213.399872	10394.495825	26.750887
213.302850	10390.585918	26.755904
213.614198	10404.900574	26.760922
213.689119	10422.858206	26.765940
213.952105	10421.006251	26.770957
214.052092	10422.387320	26.775975
213.650346	10440.626176	26.780992
214.448917	10456.557169	26.786010
214.201887	10462.869322	26.791028
214.666048	10478.048154	26.796045
214.826537	10478.322696	26.801063
214.644023	10502.520897	26.806080
214.893666	10519.131089	26.811098
215.123205	10545.756844	26.816116
215.043582	10552.859052	26.821133
215.445022	10574.745742	26.826151
215.768825	10595.431373	26.831168
216.040608	10609.803953	26.836186
215.940780	10632.823611	26.841204
216.217114	10654.997341	26.846221
216.804276	10674.050670	26.851239
216.731178	10705.605232	26.856256
217.084002	10721.297399	26.861274
217.638581	10726.153000	26.866292
218.171358	10745.197283	26.871309
218.549107	10751.080192	26.876327
218.461472	10769.839433	26.881344
219.037914	10766.015103	26.886362
219.027425	10777.937289	26.891380
219.283882	10787.427691	26.896397
219.808038	10793.985954	26.901415
219.653728	10820.966269	26.906432
219.802054	10819.551512	26.911450
219.646721	10833.385925	26.916468
220.122215	10848.668010	26.921485
220.323254	10867.693987	26.926503
220.305095	10883.570498	26.931520
220.626180	10915.258860	26.936538
221.086559	10915.110464	26.941556
220.878990	10940.046083	26.946573
221.116268	10958.153949	26.951591
221.334930	10980.989929	26.956608
221.513150	10984.597738	26.961626
221.544423	11017.741136	26.966644
221.747761	11032.328648	26.971661
222.143008	11056.277035	26.976679
222.190783	11088.856174	26.981696
222.373228	11098.204585	26.986714
222.958187	11126.858602	26.991732
223.195586	11154.852432	26.996749
223.938670	11156.210817	27.001767
224.023252	11175.990607	27.006784
224.429701	11183.933693	27.011802
224.513076	11197.235833	27.016820
224.614996	11222.692681	27.021837
224.755208	11220.002244	27.026855
225.113664	11234.694295	27.031872
225.326228	11251.123096	27.036890
225.517720	11270.089681	27.041908
225.812211	11274.201432	27.046925
226.191538	11298.166203	27.051943
226.433923	11309.029191	27.056960
226.253973	11320.859248	27.061978
226.584531	11339.969161	27.066996
226.805808	11351.665989	27.072013
226.574693	11364.665724	27.077031
226.917441	11391.822478	27.082048
227.450748	11404.998459	27.087066
227.818662	11425.497472	27.092084
228.162588	11439.851789	27.097101
228.297179	11457.342229	27.102119
228.478111	11464.839801	27.107136
228.914812	11481.272771	27.112154
229.015822	11494.695926	27.117172
229.165297	11497.941491	27.122189
229.750597	11505.510924	27.127207
229.780128	11517.177317	27.132224
229.878973	11527.812075	27.137242
229.904428	11537.188256	27.142260
229.767078	11558.105730	27.147277
230.452834	11572.091723	27.152295
230.150437	11584.625221	27.157312
230.152326	11592.647957	27.162330
230.193842	11627.527221	27.167348
230.562260	11648.549533	27.172365
231.236641	11669.871106	27.177383
231.107893	11706.666239	27.182400
231.497703	11722.754268	27.187418
232.088651	11744.780627	27.192436
232.372577	11765.717002	27.197453
232.818241	11773.218248	27.202471
232.739372	11799.611067	27.207488
232.891797	11811.172286	27.212506
233.444369	11824.421059	27.217524
233.427402	11853.186854	27.222541
233.726266	11858.202437	27.227559
234.135355	11891.733478	27.232576
234.338132	11900.965554	27.237594
234.959304	11924.179911	27.242612
234.940083	11934.954981	27.247629
235.280656	11939.556400	27.252647
235.562678	11964.025111	27.257664
235.805579	11970.293934	27.262682
235.944031	11983.860996	27.267700
235.807392	11995.867165	27.272717
236.364986	12010.787006	27.277735
236.610248	12028.814406	27.282752
236.765172	12041.546861	27.287770
236.984078	12058.455221	27.292788
237.316728	12077.464039	27.297805
237.695757	12094.893516	27.302823
237.764025	12109.691825	27.307840
238.032605	12133.765954	27.312858
238.313429	12133.858355	27.317876
238.407147	12168.083364	27.322893
238.532854	12169.495000	27.327911
238.986347	12200.303720	27.332928
239.136313	12208.891592	27.337946
239.376489	12223.289750	27.342964
239.263561	12241.698000	27.347981
239.595118	12256.460035	27.352999
239.772292	12292.036036	27.358016
240.176334	12303.365383	27.363034
240.488797	12326.931490	27.368052
240.400255	12346.251290	27.373069
240.942976	12366.318466	27.378087
240.878276	12394.881186	27.383104
241.073565	12410.679820	27.388122
241.530961	12428.876668	27.393140
241.653680	12457.982868	27.398157
242.368986	12462.256238	27.403175
242.408495	12491.237586	27.408192
242.857923	12506.975418	27.413210
243.382414	12503.395623	27.418228
243.389930	12523.341854	27.423245
243.912292	12519.316489	27.428263
244.362798	12547.005730	27.433280
244.492720	12547.628862	27.438298
244.770796	12573.469209	27.443316
244.811807	12584.200883	27.448333
245.437830	12577.279597	27.453351
245.458913	12585.137360	27.458368
245.628049	12601.589685	27.463386
245.866809	12599.297144	27.468404
245.798958	12603.877996	27.473421
245.966913	12607.583198	27.478439
246.071081	12632.053947	27.483456
246.128536	12645.028306	27.488474
246.396550	12669.823422	27.493492
246.212838	12690.995044	27.498509
246.610432	12708.284246	27.503527
246.882632	12737.601033	27.508544
247.445530	12756.363044	27.513562
247.817491	12776.869416	27.518580
247.490536	12798.129448	27.523597
247.624383	12809.104350	27.528615
247.983288	12840.447543	27.533632
248.223007	12871.693885	27.538650
249.012914	12873.689163	27.543668
249.100818	12904.273639	27.548685
249.456550	12922.535902	27.553703
249.812788	12946.584157	27.558720
250.094875	12958.372954	27.563738
250.470888	12980.416822	27.568756
250.381239	13002.684198	27.573773
250.739077	13008.335661	27.578791
251.362603	13015.455930	27.583808
251.491189	13034.088327	27.588826
251.790534	13050.726019	27.593844
251.623057	13073.012653	27.598861
252.096223	13089.087491	27.603879
252.360833	13107.552532	27.608896
252.490436	13129.916221	27.613914
253.168158	13140.722706	27.618932
253.343508	13163.110398	27.623949
253.611307	13182.178507	27.628967
253.885642	13193.740273	27.633984
253.748023	13208.486939	27.639002
254.024868	13223.756050	27.644020
254.397412	13246.437458	27.649037
254.575434	13255.352160	27.654055
254.999200	13280.308420	27.659072
255.132646	13304.841531	27.664090
255.483863	13309.994679	27.669108
255.879961	13326.868791	27.674125
255.990343	13353.118638	27.679143
256.301355	13363.913374	27.684160
256.478391	13392.698706	27.689178
256.689098	13396.189026	27.694196
256.430169	13421.554539	27.699213
257.117721	13435.065194	27.704231
257.366535	13468.529873	27.709248
257.719284	13492.138299	27.714266
257.937267	13499.625184	27.719284
258.098148	13529.563746	27.724301
258.147373	13543.832326	27.729319
258.473041	13564.700323	27.734336
258.851789	13595.253810	27.739354
259.012314	13615.028771	27.744372
259.429226	13640.801402	27.749389
259.866702	13649.957099	27.754407
259.996154	13671.760579	27.759424
260.410814	13686.090246	27.764442
260.678648	13703.206554	27.769460
260.570670	13730.232136	27.774477
260.811749	13745.707775	27.779495
261.279112	13763.746117	27.784512
261.511467	13775.505908	27.789530
261.895572	13801.147120	27.794548
262.175122	13820.965700	27.799565
262.343767	13834.036101	27.804583
262.599087	13843.915359	27.809600
262.573447	13869.047627	27.814618
263.110375	13875.315891	27.819636
263.168091	13900.207518	27.824653
263.469032	13924.365640	27.829671
264.020523	13927.587038	27.834688
264.062852	13955.981186	27.839706
264.410709	13968.172720	27.844724
264.772651	13995.452029	27.849741
264.477752	14016.662659	27.854759
264.795794	14026.416630	27.859776
264.925401	14070.041125	27.864794
265.387118	14082.752868	27.869812
265.780840	14103.104473	27.874829
266.010324	14133.923163	27.879847
266.451195	14148.026715	27.884864
266.597319	14178.290384	27.889882
266.877105	14194.089407	27.894900
267.228478	14207.192954	27.899917
267.810574	14229.250177	27.904935
268.033552	14250.758483	27.909952
268.473392	14258.123970	27.914970
268.850138	14277.366048	27.919988
269.027524	14295.416647	27.925005
268.862338	14300.308742	27.930023
269.464856	14317.953472	27.935040
269.539161	14338.964849	27.940058
270.060931	14361.843786	27.945076
270.080107	14387.295654	27.950093
270.344134	14397.102897	27.955111
270.682637	14414.859113	27.960128
270.650195	14436.395681	27.965146
271.160091	14450.587373	27.970164
271.291668	14488.520627	27.975181
271.411425	14507.293277	27.980199
271.774841	14531.883226	27.985216
271.957307	14548.475580	27.990234
272.243436	14573.371475	27.995252
272.657745	14604.417390	28.000269
272.927248	14631.818625	28.005287
273.290320	14644.952110	28.010304
273.548450	14667.057149	28.015322
273.776213	14682.606797	28.020340
273.956995	14716.931542	28.025357
274.035711	14736.855336	28.030375
274.596305	14754.778523	28.035392
274.620500	14788.606091	28.040410
275.137586	14824.358424	28.045428
275.176240	14836.278635	28.050445
275.181463	14863.539540	28.055463
275.907888	14884.101911	28.060480
275.848837	14904.890207	28.065498
276.817832	14920.791973	28.070516
277.230993	14938.577402	28.075533
277.218076	14959.288806	28.080551
278.002082	14976.667882	28.085568
277.829107	14995.743180	28.090586
278.417246	15003.588803	28.095604
278.682293	15020.019858	28.100621
278.846209	15048.271326	28.105639
278.980945	15052.187449	28.110656
279.345271	15083.734227	28.115674
279.935963	15089.157265	28.120692
280.069807	15096.184434	28.125709
279.983389	15126.957912	28.130727
280.346443	15128.798651	28.135744
280.413817	15165.273740	28.140762
280.531957	15175.003120	28.145780
281.033477	15200.176424	28.150797
280.922742	15226.568262	28.155815
281.288064	15232.644776	28.160832
281.491433	15265.677822	28.165850
281.513292	15295.856932	28.170868
281.772006	15317.735821	28.175885
281.553295	15357.208786	28.180903
282.148284	15382.497734	28.185920
282.392499	15426.188875	28.190938
282.658928	15450.282470	28.195956
282.915194	15487.220348	28.200973
283.230547	15516.763541	28.205991
284.105205	15540.324968	28.211008
284.113532	15573.271085	28.216026
284.605593	15604.484147	28.221044
285.158897	15627.915978	28.226061
285.246753	15649.661213	28.231079
285.854909	15669.082616	28.236096
285.907976	15694.483643	28.241114
285.836228	15727.633994	28.246132
286.215247	15741.895718	28.251149
286.472224	15780.321879	28.256167
287.081045	15803.856687	28.261184
287.493650	15836.266895	28.266202
287.743628	15861.331480	28.271220
288.139726	15874.492024	28.276237
288.403288	15911.733824	28.281255
288.834706	15933.540877	28.286272
289.119194	15953.939637	28.291290
289.289449	15973.083873	28.296308
289.526816	15981.785386	28.301325
289.946209	16007.915963	28.306343
290.446649	16036.208103	28.311360
290.549262	16053.176089	28.316378
290.380241	16077.906767	28.321396
290.822798	16092.752463	28.326413
291.040847	16127.691818	28.331431
291.729293	16147.899576	28.336448
291.617481	16174.156003	28.341466
292.065691	16202.813244	28.346484
292.803235	16220.546481	28.351501
292.716667	16257.612083	28.356519
293.066451	16273.849156	28.361536
293.221752	16294.882765	28.366554
293.596659	16319.237104	28.371572
293.730605	16344.983541	28.376589
293.997794	16379.461411	28.381607
294.411739	16403.476879	28.386624
294.735453	16429.015577	28.391642
295.056923	16448.209462	28.396660
295.310004	16478.978248	28.401677
295.383269	16518.044850	28.406695
296.037951	16519.285948	28.411712
296.157701	16547.528388	28.416730
296.346716	16575.333893	28.421748
296.623192	16592.232736	28.426765
296.980529	16637.307974	28.431783
297.097288	16648.828886	28.436800
297.261812	16684.180169	28.441818
297.819937	16724.823626	28.446836
298.304831	16735.959106	28.451853
298.316922	16779.665411	28.456871
298.612087	16797.496001	28.461888
299.369738	16826.358538	28.466906
299.538553	16854.572910	28.471924
300.186610	16876.424235	28.476941
300.136260	16888.333850	28.481959
300.585668	16912.815460	28.486976
300.856124	16924.464056	28.491994
301.081706	16956.161878	28.497012
301.414537	16975.898261	28.502029
301.427572	16998.678966	28.507047
301.842214	17024.384822	28.512064
302.342547	17044.746129	28.517082
301.999870	17062.341941	28.522100
302.499598	17103.437296	28.527117
302.729509	17119.791156	28.532135
303.122295	17133.870566	28.537152
303.037437	17172.652773	28.542170
303.203486	17195.637010	28.547188
303.916337	17228.487393	28.552205
304.253140	17275.136028	28.557223
304.690333	17300.083619	28.562240
305.032184	17327.100717	28.567258
305.079156	17358.072271	28.572276
305.767818	17378.365051	28.577293
306.148754	17400.500779	28.582311
306.332098	17434.361102	28.587328
306.636090	17466.168316	28.592346
306.927300	17500.721803	28.597364
307.195571	17509.623924	28.602381
307.326073	17542.044703	28.607399
307.553193	17573.344690	28.612416
307.893488	17604.008179	28.617434
308.127359	17628.915779	28.622452
308.657199	17658.137379	28.627469
308.736843	17699.697667	28.632487
309.337400	17723.577057	28.637504
309.662669	17752.720712	28.642522
310.293277	17787.488257	28.647540
311.185056	17791.404489	28.652557
311.400152	17816.320203	28.657575
311.949338	17821.678515	28.662592
312.254536	17849.277835	28.667610
312.492009	17855.154209	28.672628
312.843451	17867.824079	28.677645
313.132167	17891.471515	28.682663
313.123430	17900.098066	28.687680
313.493271	17922.609890	28.692698
313.723390	17938.991325	28.697716
314.084514	17947.384992	28.702733
313.968029	17989.492255	28.707751
314.551038	18006.267830	28.712768
314.907716	18029.390392	28.717786
315.282084	18053.840388	28.722804
315.792271	18062.212641	28.727821
315.860917	18092.474272	28.732839
316.232911	18106.140253	28.737856
316.413511	18126.117532	28.742874
316.811300	18167.347448	28.747892
317.193354	18178.081624	28.752909
317.255477	18191.857189	28.757927
317.146193	18223.850781	28.762944
317.407360	18259.205240	28.767962
317.727200	18291.645076	28.772980
318.115570	18312.790925	28.777997
318.941715	18339.181144	28.783015
319.182843	18370.699427	28.788032
319.557609	18385.451215	28.793050
319.358843	18412.537337	28.798068
320.069990	18437.050483	28.803085
320.224550	18470.116949	28.808103
320.435631	18494.102782	28.813120
320.818683	18515.164652	28.818138
321.338001	18545.048440	28.823156
321.708731	18559.211529	28.828173
322.184298	18586.344159	28.833191
322.279404	18609.603745	28.838208
322.522126	18624.171070	28.843226
322.842487	18650.404176	28.848244
323.277706	18670.909084	28.853261
323.304984	18701.363086	28.858279
323.166467	18723.781865	28.863296
323.997619	18747.900495	28.868314
324.308042	18788.076096	28.873332
324.863451	18813.640116	28.878349
325.147604	18838.002143	28.883367
325.406473	18850.806285	28.888384
326.149151	18872.977231	28.893402
326.039242	18910.864436	28.898420
326.201551	18918.935202	28.903437
326.380930	18944.135945	28.908455
326.932835	18988.126191	28.913472
327.297908	19002.727232	28.918490
327.756023	19034.270830	28.923508
328.103767	19071.455426	28.928525
328.071838	19088.048380	28.933543
327.921008	19121.765596	28.938560
328.387511	19148.755625	28.943578
329.079610	19195.636300	28.948596
329.073579	19216.304630	28.953613
329.458167	19249.935230	28.958631
329.863047	19295.496960	28.963648
330.409478	19322.866575	28.968666
330.408038	19365.029259	28.973684
331.126943	19395.283576	28.978701
331.403386	19423.511353	28.983719
331.571711	19461.155228	28.988736
332.027661	19477.776740	28.993754
331.903225	19518.170973	28.998772
332.811662	19556.004913	29.003789
333.313627	19586.667439	29.008807
333.466975	19613.440401	29.013824
334.122316	19637.888883	29.018842
334.215036	19673.887393	29.023860
334.292007	19703.379742	29.028877
335.237142	19739.016881	29.033895
335.387354	19769.745738	29.038912
335.735963	19797.014824	29.043930
335.762841	19833.994031	29.048948
336.274365	19862.814271	29.053965
336.559104	19882.644047	29.058983
336.532396	19913.861126	29.064000
337.055629	19950.200550	29.069018
337.501987	19984.895958	29.074036
337.869050	20018.896734	29.079053
338.129738	20052.153750	29.084071
338.467598	20087.885654	29.089088
338.944444	20111.717995	29.094106
339.286509	20150.991535	29.099124
339.356662	20185.703795	29.104141
339.671626	20219.686789	29.109159
340.062033	20255.410372	29.114176
340.464443	20277.743457	29.119194
341.034579	20323.758360	29.124212
341.373757	20348.871775	29.129229
341.599927	20385.683708	29.134247
341.956955	20411.886740	29.139264
342.566017	20433.777598	29.144282
342.730045	20470.437611	29.149300
342.803160	20490.594713	29.154317
343.608073	20528.406983	29.159335
343.795525	20550.358186	29.164352
344.144751	20566.970045	29.169370
344.679126	20602.449885	29.174388
345.253260	20620.851756	29.179405
345.616130	20635.656384	29.184423
345.633586	20659.103498	29.189440
346.141951	20676.773782	29.194458
346.066231	20705.684613	29.199476
346.397066	20728.268173	29.204493
346.769777	20753.264728	29.209511
347.040600	20793.566797	29.214528
347.340083	20803.234857	29.219546
347.773232	20849.995868	29.224564
348.020221	20873.662330	29.229581
348.353522	20905.624218	29.234599
348.405335	20939.038896	29.239616
348.921292	20973.513615	29.244634
349.306998	21009.040950	29.249652
349.738153	21049.879959	29.254669
349.983232	21082.039632	29.259687
350.098531	21122.208958	29.264704
350.655109	21159.247054	29.269722
350.882027	21197.665539	29.274740
351.262636	21230.213000	29.279757
351.786688	21269.701890	29.284775
351.879743	21310.966295	29.289792
352.542841	21337.363001	29.294810
353.174056	21372.267236	29.299828
353.263655	21409.818153	29.304845
354.086098	21433.300480	29.309863
354.456163	21465.848565	29.314880
354.533225	21504.333499	29.319898
355.013540	21530.655078	29.324916
355.046511	21574.558156	29.329933
355.649685	21590.258827	29.334951
355.392694	21628.452389	29.339968
355.983248	21668.230778	29.344986
356.210018	21706.246854	29.350004
356.524882	21746.668488	29.355021
357.081362	21787.725077	29.360039
357.141343	21832.909271	29.365056
357.389880	21864.483389	29.370074
357.852613	21903.231875	29.375092
358.676101	21948.186196	29.380109
358.951620	21983.484700	29.385127
358.788440	22042.112041	29.390144
359.673405	22072.419465	29.395162
359.838274	22101.920440	29.400180
360.053838	22155.325405	29.405197
360.924175	22185.425762	29.410215
360.780284	22245.838496	29.415232
361.845687	22257.597586	29.420250
363.072532	22274.945912	29.425268
363.175692	22312.903373	29.430285
363.633650	22328.057991	29.435303
364.311162	22340.043610	29.440320
365.127053	22352.914512	29.445338
365.405322	22358.005317	29.450356
365.646963	22376.867666	29.455373
366.337793	22398.261994	29.460391
365.938321	22387.249185	29.465408
366.666844	22415.803067	29.470426
366.890470	22429.350490	29.475444
366.937432	22438.473130	29.480461
367.647066	22469.273767	29.485479
367.410991	22496.694297	29.490496
367.743863	22517.857810	29.495514
367.844500	22545.894443	29.500532
367.922095	22562.480631	29.505549
368.505521	22583.233902	29.510567
368.437063	22622.552675	29.515584
368.650938	22663.507185	29.520602
368.889383	22690.737698	29.525620
369.280302	22735.068705	29.530637
369.464614	22761.985061	29.535655
369.281181	22814.996070	29.540672
369.877585	22861.338397	29.545690
370.209633	22904.862861	29.550708
370.477997	22952.952976	29.555725
370.643673	22996.757429	29.560743
371.043007	23049.289768	29.565760
371.591612	23095.801457	29.570778
372.511910	23143.026030	29.575796
372.701536	23180.283720	29.580813
373.173695	23224.962080	29.585831
373.784613	23267.083869	29.590848
374.221929	23298.211663	29.595866
374.464242	23337.340433	29.600884
374.759392	23388.503531	29.605901
375.145379	23428.179549	29.610919
375.650268	23473.001370	29.615936
375.925682	23507.547833	29.620954
376.722343	23546.285933	29.625972
376.812704	23595.176726	29.630989
377.301270	23625.729033	29.636007
377.638070	23664.956477	29.641024
377.827945	23700.408324	29.646042
378.678565	23738.305429	29.651060
378.783006	23782.812649	29.656077
379.268562	23810.899744	29.661095
379.458708	23863.210580	29.666112
379.817570	23900.514430	29.671130
380.565442	23937.101318	29.676148
380.423037	23990.287402	29.681165
380.964049	24019.254982	29.686183
381.392256	24061.497233	29.691200
381.559681	24113.383710	29.696218
382.452117	24147.750711	29.701236
382.510843	24192.618182	29.706253
382.748717	24225.382650	29.711271
383.239639	24277.175192	29.716288
383.451182	24318.020562	29.721306
383.994037	24350.288655	29.726324
384.417849	24400.960513	29.731341
385.225342	24436.783339	29.736359
385.323722	24482.487044	29.741376
385.951733	24520.846841	29.746394
386.722556	24552.122105	29.751412
386.439462	24603.895284	29.756429
387.589451	24640.442494	29.761447
388.411920	24664.470191	29.766464
388.584053	24695.325840	29.771482
388.913770	24714.784910	29.776500
388.905183	24757.556755	29.781517
389.267126	24772.798816	29.786535
389.644888	24828.668959	29.791552
389.804160	24869.579479	29.796570
390.213938	24883.659479	29.801588
390.537595	24929.732424	29.806605
390.891409	24964.011873	29.811623
391.320872	25005.832090	29.816640
391.516212	25049.979125	29.821658
392.388781	25083.671676	29.826676
392.709946	25123.294562	29.831693
392.855877	25159.321235	29.836711
393.250529	25189.295812	29.841728
393.261652	25230.506049	29.846746
393.917722	25261.576083	29.851764
394.199917	25307.483441	29.856781
395.105638	25327.105094	29.861799
395.528564	25367.334612	29.866816
395.645010	25393.194064	29.871834
396.132781	25421.362305	29.876852
396.742491	25461.610074	29.881869
397.348643	25490.145217	29.886887
397.537177	25510.237207	29.891904
397.960626	25539.930108	29.896922
398.432019	25569.418025	29.901940
398.477228	25598.801357	29.906957
398.917129	25643.865146	29.911975
399.323696	25675.477037	29.916992
399.726895	25711.235300	29.922010
400.136009	25744.267715	29.927028
400.082307	25786.800437	29.932045
400.497347	25828.445283	29.937063
401.002082	25877.143295	29.942080
401.348285	25909.719646	29.947098
402.126719	25943.167677	29.952116
402.321214	25993.733922	29.957133
402.951788	26024.793791	29.962151
403.123499	26071.345930	29.967168
403.391774	26112.306078	29.972186
403.804803	26149.016123	29.977204
404.132332	26194.063655	29.982221
404.461681	26241.312472	29.987239
404.629048	26283.576516	29.992256
404.882494	26337.414167	29.997274
405.278051	26384.292888	30.002292
405.914782	26443.460881	30.007309
406.129981	26482.494125	30.012327
406.729538	26541.703293	30.017344
406.895666	26603.917511	30.022362
407.718940	26637.589739	30.027380
408.221789	26692.860243	30.032397
408.674589	26735.854146	30.037415
409.063528	26786.377992	30.042432
409.426704	26827.005611	30.047450
410.007202	26874.334540	30.052468
410.350332	26911.117692	30.057485
410.776204	26959.260920	30.062503
411.288174	27012.080213	30.067520
411.100999	27054.710670	30.072538
411.881632	27105.530321	30.077556
412.239558	27153.802020	30.082573
412.933824	27202.759517	30.087591
413.252911	27251.993612	30.092608
413.561188	27296.498397	30.097626
414.278328	27344.228707	30.102644
414.660858	27380.498535	30.107661
414.914094	27423.646984	30.112679
415.527148	27463.099325	30.117696
415.609501	27515.852350	30.122714
416.314289	27559.923277	30.127732
416.417657	27601.945644	30.132749
416.935086	27649.082102	30.137767
417.664304	27696.606370	30.142784
417.835260	27736.974548	30.147802
418.391128	27781.048561	30.152820
418.770513	27839.210355	30.157837
419.219569	27870.492811	30.162855
419.562221	27922.424978	30.167872
419.711368	27966.733828	30.172890
420.211234	28019.227013	30.177908
421.003954	28059.956919	30.182925
421.458890	28085.059527	30.187943
421.767200	28123.462870	30.192960
421.934618	28167.759755	30.197978
422.387431	28203.117571	30.202996
422.528046	28246.766140	30.208013
422.742225	28286.421893	30.213031
423.474016	28336.486744	30.218048
423.754828	28391.931864	30.223066
425.087207	28420.094845	30.228084
425.955162	28457.539037	30.233101
426.123077	28491.014030	30.238119
426.486082	28518.848372	30.243136
426.441276	28561.168827	30.248154
426.956444	28603.945750	30.253172
427.311799	28635.377555	30.258189
427.266417	28687.527532	30.263207
428.297852	28725.024159	30.268224
428.402734	28773.083528	30.273242
428.623184	28814.606876	30.278260
428.980809	28865.315483	30.283277
429.687103	28910.714481	30.288295
430.049995	28965.920761	30.293312
429.936397	29006.436695	30.298330
430.459086	29070.780648	30.303348
430.771482	29112.778468	30.308365
431.177217	29174.085424	30.313383
431.950427	29217.590936	30.318400
432.214898	29286.145447	30.323418
432.728720	29324.432336	30.328436
433.045745	29379.095465	30.333453
433.569403	29428.872942	30.338471
434.406839	29490.078158	30.343488
434.565261	29541.310603	30.348506
435.199832	29588.581263	30.353524
435.653993	29650.105876	30.358541
435.919581	29691.548157	30.363559
436.549633	29746.633924	30.368576
436.745458	29797.816781	30.373594
437.476330	29842.015404	30.378612
438.263085	29887.277483	30.383629
438.563337	29945.938926	30.388647
438.845955	29979.019286	30.393664
439.219172	30039.088580	30.398682
439.354304	30076.515367	30.403700
440.372770	30124.506429	30.408717
440.718299	30173.911665	30.413735
441.510686	30221.060183	30.418752
441.480890	30276.143054	30.423770
442.024202	30313.301024	30.428788
442.820701	30360.786794	30.433805
442.933220	30421.764863	30.438823
443.649906	30459.670569	30.443840
443.830187	30517.306381	30.448858
443.932886	30557.496802	30.453876
444.812312	30600.429843	30.458893
444.956145	30653.952013	30.463911
445.452797	30696.405898	30.468928
445.992358	30741.505972	30.473946
446.647244	30793.896765	30.478964
446.829858	30834.727666	30.483981
447.257036	30888.244762	30.488999
447.590942	30949.046134	30.494016
448.072789	30996.670792	30.499034
448.612481	31040.146878	30.504052
449.176669	31096.736876	30.509069
449.352434	31139.471992	30.514087
450.081636	31176.373945	30.519104
450.373190	31238.334843	30.524122
450.941431	31281.914080	30.529140
451.711005	31316.841016	30.534157
452.170446	31373.799406	30.539175
452.327953	31396.857928	30.544192
453.004501	31435.501167	30.549210
453.331768	31490.068263	30.554228
453.611614	31521.151784	30.559245
454.408480	31571.369798	30.564263
454.924151	31604.727079	30.569280
454.890877	31658.843154	30.574298
455.279892	31694.717092	30.579316
455.854562	31727.784072	30.584333
456.273706	31786.154415	30.589351
456.967872	31829.960304	30.594368
457.518262	31873.591288	30.599386
457.466325	31926.070676	30.604404
458.107227	31969.809992	30.609421
458.526653	32011.285998	30.614439
459.187197	32057.741910	30.619456
459.254318	32104.668261	30.624474
459.624275	32160.637532	30.629492
460.352515	32209.625625	30.634509
460.242434	32266.223504	30.639527
460.727791	32319.946750	30.644544
461.538107	32379.434445	30.649562
461.873213	32443.427427	30.654580
462.195851	32494.319573	30.659597
462.390936	32555.316661	30.664615
463.283957	32612.999383	30.669632
463.922046	32671.752977	30.674650
463.961959	32739.272747	30.679668
464.612769	32796.194672	30.684685
464.880880	32856.287831	30.689703
465.357294	32913.185302	30.694720
466.046664	32986.237035	30.699738
466.489084	33031.299093	30.704756
467.222555	33097.686544	30.709773
467.233623	33153.084052	30.714791
468.041802	33204.342931	30.719808
468.633886	33260.686028	30.724826
469.504611	33312.692147	30.729844
470.353818	33354.116101	30.734861
470.710452	33414.477355	30.739879
470.979301	33457.152240	30.744896
472.008269	33502.336329	30.749914
472.034433	33551.500918	30.754932
472.672587	33592.774132	30.759949
472.830544	33648.458147	30.764967
473.280184	33685.010828	30.769984
473.846039	33733.452559	30.775002
474.129497	33793.836659	30.780020
475.073380	33831.667952	30.785037
475.355651	33874.016625	30.790055
475.569959	33926.233948	30.795072
476.406387	33969.150783	30.800090
476.753548	34022.769514	30.805108
477.364095	34063.827512	30.810125
477.617146	34119.579340	30.815143
477.772692	34174.445004	30.820160
478.220397	34220.190785	30.825178
478.625753	34290.587480	30.830196
479.074546	34339.807506	30.835213
479.595381	34397.781572	30.840231
480.119968	34454.392054	30.845248
480.208118	34511.869981	30.850266
480.666873	34562.641464	30.855284
481.624928	34630.414372	30.860301
481.586582	34685.815363	30.865319
482.104736	34733.945846	30.870336
482.748071	34788.549815	30.875354
483.078231	34850.352927	30.880372
483.781476	34899.942692	30.885389
483.899176	34958.408015	30.890407
484.491278	34998.657094	30.895424
485.263118	35069.274025	30.900442
485.844671	35119.275791	30.905460
486.403190	35166.583487	30.910477
486.830579	35214.831243	30.915495
487.364153	35275.781780	30.920512
487.719434	35324.335213	30.925530
488.121380	35379.621454	30.930548
488.738648	35427.361924	30.935565
488.911259	35485.671591	30.940583
489.479753	35551.319191	30.945600
489.830143	35613.052182	30.950618
490.076497	35674.824659	30.955636
490.909519	35742.379468	30.960653
491.170836	35800.363097	30.965671
491.879595	35861.012152	30.970688
492.385872	35923.190663	30.975706
492.940298	35990.016122	30.980724
493.183635	36049.647659	30.985741
493.746230	36107.140717	30.990759
494.220653	36187.193213	30.995776
494.991280	36237.002781	31.000794
495.127983	36315.170838	31.005812
495.878961	36373.959063	31.010829
496.666103	36428.837787	31.015847
497.020210	36498.084012	31.020864
497.055005	36555.624663	31.025882
497.729331	36614.887088	31.030900
498.600741	36693.301514	31.035917
499.504494	36750.077557	31.040935
499.706246	36805.215074	31.045952
500.339808	36857.778830	31.050970
501.202803	36923.524833	31.055988
501.567107	36973.816985	31.061005
502.303124	37026.361156	31.066023
502.514386	37083.094840	31.071040
503.085440	37127.022515	31.076058
503.238975	37183.860730	31.081076
503.938964	37241.722910	31.086093
504.292520	37298.711494	31.091111
504.692761	37362.727180	31.096128
505.355638	37421.946821	31.101146
505.775330	37483.059386	31.106164
506.117469	37537.671002	31.111181
506.576833	37600.598419	31.116199
507.183852	37666.540908	31.121216
508.112212	37728.671736	31.126234
508.863876	37787.795858	31.131252
509.689022	37823.755309	31.136269
510.141159	37871.567438	31.141287
510.683641	37922.666008	31.146304
511.174582	37970.572984	31.151322
511.418389	38027.941792	31.156340
511.715928	38071.743366	31.161357
512.311807	38131.711773	31.166375
512.380771	38189.974745	31.171392
513.270623	38238.012220	31.176410
513.801822	38295.981413	31.181428
514.189209	38345.910627	31.186445
514.633514	38413.770089	31.191463
515.046226	38474.615735	31.196480
515.739525	38530.213883	31.201498
515.720833	38591.999124	31.206516
516.584288	38637.176215	31.211533
516.517067	38697.281274	31.216551
517.166359	38760.841006	31.221568
517.622435	38815.039981	31.226586
517.686187	38886.486405	31.231604
518.371827	38939.145471	31.236621
518.900748	39008.274614	31.241639
519.484308	39091.591855	31.246656
520.106920	39150.628126	31.251674
520.087513	39212.058937	31.256692
520.758644	39273.754653	31.261709
521.540076	39356.838425	31.266727
521.648324	39427.440048	31.271744
522.522424	39504.063984	31.276762
522.862275	39576.285005	31.281780
523.709854	39630.213431	31.286797
523.947937	39711.810393	31.291815
524.699558	39790.639974	31.296832
525.466476	39848.057546	31.301850
526.036579	39910.677996	31.306868
526.486112	39978.832832	31.311885
526.921441	40049.468065	31.316903
527.471502	40127.581166	31.321920
528.091320	40189.619891	31.326938
528.387601	40263.542690	31.331956
529.017862	40335.529365	31.336973
529.462122	40402.727087	31.341991
530.302861	40476.835436	31.347008
530.730514	40541.195559	31.352026
531.382826	40603.470218	31.357044
532.227360	40669.444365	31.362061
532.779981	40743.228912	31.367079
533.226151	40812.668975	31.372096
534.017016	40869.555507	31.377114
534.702193	40934.389001	31.382132
535.226800	40989.817352	31.387149
535.857276	41054.319394	31.392167
536.047150	41128.013891	31.397184
536.719946	41166.969198	31.402202
537.129866	41240.141681	31.407220
537.657694	41297.423375	31.412237
537.917588	41361.855129	31.417255
538.320376	41450.639289	31.422272
539.196417	41509.262536	31.427290
539.368011	41578.652994	31.432308
540.052816	41646.967744	31.437325
540.784739	41714.312168	31.442343
541.084781	41790.901619	31.447360
542.079431	41848.445700	31.452378
542.208006	41923.646649	31.457396
543.169819	41984.861568	31.462413
543.386706	42056.055171	31.467431
543.800463	42125.682335	31.472448
544.519195	42195.916003	31.477466
544.954927	42253.698881	31.482484
545.643720	42327.530443	31.487501
546.486878	42399.550039	31.492519
546.884039	42464.086097	31.497536
547.307455	42519.892503	31.502554
548.127577	42591.297910	31.507572
548.336624	42650.053903	31.512589
549.670863	42714.101434	31.517607
550.014258	42772.406290	31.522624
550.748825	42831.016080	31.527642
551.139541	42899.412464	31.532660
551.853904	42953.271663	31.537677
552.469834	43005.186820	31.542695
552.591222	43080.090604	31.547712
552.984802	43118.546857	31.552730
553.407007	43180.056919	31.557748
553.910378	43250.794249	31.562765
554.774677	43298.211557	31.567783
554.952537	43366.142863	31.572800
555.213829	43428.343296	31.577818
555.728981	43487.802760	31.582836
556.241236	43558.375632	31.587853
556.950187	43629.112023	31.592871
557.205841	43702.262929	31.597888
557.938869	43769.179000	31.602906
558.354820	43844.826488	31.607924
558.823164	43915.521626	31.612941
559.252048	43982.782311	31.617959
559.633192	44059.954989	31.622976
560.855581	44123.151359	31.627994
561.443874	44206.431042	31.633012
561.655696	44285.343792	31.638029
562.674338	44345.310075	31.643047
563.250203	44418.458270	31.648064
564.053246	44485.138041	31.653082
564.575076	44562.213794	31.658100
564.971703	44617.390031	31.663117
565.836122	44680.085438	31.668135
566.268011	44766.512793	31.673152
567.093883	44828.078461	31.678170
568.043825	44890.864642	31.683188
568.106748	44952.414655	31.688205
568.746804	45013.812719	31.693223
569.261820	45089.234208	31.698240
569.729366	45145.663210	31.703258
570.321511	45225.720055	31.708276
570.417301	45293.978211	31.713293
571.082754	45355.167977	31.718311
571.587230	45443.209344	31.723328
572.036367	45512.335040	31.728346
572.813051	45595.810828	31.733364
573.235325	45676.510189	31.738381
573.841039	45750.596419	31.743399
574.206397	45843.581877	31.748416
574.783311	45919.372221	31.753434
575.293983	46002.047564	31.758452
576.031078	46090.306148	31.763469
576.845016	46160.747478	31.768487
577.193283	46259.310753	31.773504
577.892136	46336.213022	31.778522
578.339090	46404.032003	31.783540
578.631071	46506.243320	31.788557
579.473536	46587.751835	31.793575
580.043314	46671.023451	31.798592
580.533506	46749.859566	31.803610
581.221869	46824.908917	31.808628
581.673647	46913.610031	31.813645
582.609169	46998.701459	31.818663
583.021142	47073.601678	31.823680
583.557943	47163.316153	31.828698
584.335555	47242.915215	31.833716
584.899859	47324.422339	31.838733
585.320043	47402.900143	31.843751
585.839360	47493.825309	31.848768
586.355854	47576.383455	31.853786
587.201800	47662.446299	31.858804
587.606395	47751.266505	31.863821
588.076956	47832.510264	31.868839
588.884035	47919.846958	31.873856
589.591987	48002.255346	31.878874
590.253970	48084.839049	31.883892
590.780752	48161.278250	31.888909
591.641074	48230.721793	31.893927
591.825054	48305.465604	31.898944
592.174303	48380.507672	31.903962
593.077694	48462.191058	31.908980
593.384167	48541.374458	31.913997
594.488348	48617.896977	31.919015
594.835532	48701.040616	31.924032
595.497290	48761.427324	31.929050
596.013982	48848.860469	31.934068
596.580514	48926.420405	31.939085
597.409586	48994.109778	31.944103
597.809218	49085.690775	31.949120
598.149123	49163.064890	31.954138
598.932151	49239.535585	31.959156
599.196754	49325.983053	31.964173
599.941447	49403.708146	31.969191
600.447921	49499.922079	31.974208
601.198689	49586.865196	31.979226
601.876575	49661.122213	31.984244
602.271818	49756.970529	31.989261
602.645333	49839.953727	31.994279
603.312601	49942.636351	31.999296
603.578173	50027.308823	32.004314
604.593068	50114.182295	32.009332
605.157059	50215.977062	32.014349
606.011122	50300.149305	32.019367
606.652508	50385.231857	32.024384
607.372420	50471.741952	32.029402
608.349919	50566.001176	32.034420
608.515308	50650.538197	32.039437
609.514290	50727.149724	32.044455
610.107653	50815.529834	32.049472
610.826468	50897.162544	32.054490
611.527329	50977.181533	32.059508
612.112217	51053.758533	32.064525
612.774042	51137.053457	32.069543
613.433264	51220.614470	32.074560
614.032896	51306.405989	32.079578
614.881123	51383.165050	32.084596
615.281666	51475.521643	32.089613
615.893347	51558.599273	32.094631
616.273403	51636.690537	32.099648
616.679419	51713.075456	32.104666
617.599015	51806.933425	32.109684
617.594246	51897.760826	32.114701
618.334094	51993.051725	32.119719
618.862728	52092.616619	32.124736
619.004579	52183.057923	32.129754
620.035078	52281.991334	32.134772
620.484764	52381.093821	32.139789
620.946622	52470.403411	32.144807
621.806357	52574.619130	32.149824
622.600022	52677.589220	32.154842
623.565055	52760.784224	32.159860
623.684405	52867.391643	32.164877
624.927790	52948.216767	32.169895
625.505786	53036.758042	32.174912
626.104991	53120.867833	32.179930
627.181502	53221.096636	32.184948
627.652435	53307.256263	32.189965
627.961313	53389.317822	32.194983
629.127739	53475.988749	32.200000
629.779993	53566.055290	32.205018
630.022479	53643.510879	32.210036
630.562635	53735.131845	32.215053
631.235704	53813.685724	32.220071
631.980955	53898.172758	32.225088
632.576244	53986.494388	32.230106
633.377142	54054.894831	32.235124
633.856688	54141.966455	32.240141
634.235042	54225.270938	32.245159
634.955364	54300.470650	32.250176
635.269262	54392.725928	32.255194
636.250701	54471.199940	32.260212
636.704830	54549.717130	32.265229
637.343145	54637.093260	32.270247
638.048982	54713.124575	32.275264
638.499097	54796.451229	32.280282
639.405759	54890.089318	32.285300
639.732716	54980.348781	32.290317
640.564928	55065.736272	32.295335
641.268557	55156.667212	32.300352
641.625699	55252.122570	32.305370
642.903539	55330.765889	32.310388
642.987028	55430.727785	32.315405
643.614168	55517.300983	32.320423
644.817014	55602.459014	32.325440
644.930468	55686.969661	32.330458
645.749260	55774.156782	32.335476
646.540142	55873.050067	32.340493
647.151676	55954.946038	32.345511
647.867134	56036.168096	32.350528
648.690966	56143.928026	32.355546
649.550885	56224.564682	32.360564
649.945925	56323.487692	32.365581
650.464261	56405.520975	32.370599
651.250667	56483.207548	32.375616
652.002808	56583.349187	32.380634
652.419164	56662.159062	32.385652
653.038602	56751.493769	32.390669
654.023025	56853.165379	32.395687
654.648118	56934.260734	32.400704
655.250075	57020.307622	32.405722
655.826012	57107.502833	32.410740
656.405924	57199.411411	32.415757
657.037205	57298.053857	32.420775
657.541426	57380.529496	32.425792
658.038083	57482.158518	32.430810
659.253084	57567.007093	32.435828
660.144312	57659.555125	32.440845
660.775136	57748.342720	32.445863
661.429528	57831.376755	32.450880
661.805487	57923.865782	32.455898
662.548070	58013.425952	32.460916
663.327319	58105.735484	32.465933
663.824316	58189.580544	32.470951
664.605382	58282.509844	32.475968
665.111634	58384.211400	32.480986
665.495152	58470.869350	32.486004
666.135336	58576.423286	32.491021
666.681406	58679.787985	32.496039
667.326633	58767.137007	32.501056
668.042963	58870.727338	32.506074
668.777127	58973.891880	32.511092
669.475223	59066.680557	32.516109
669.785735	59176.039357	32.521127
670.560106	59279.641178	32.526144
671.006603	59393.749713	32.531162
671.696800	59498.522989	32.536180
672.120546	59592.970828	32.541197
673.199865	59690.401003	32.546215
673.818107	59808.749089	32.551232
674.244712	59915.533400	32.556250
675.016180	60019.404937	32.561268
675.660556	60125.718359	32.566285
676.420738	60240.133789	32.571303
676.920183	60331.551871	32.576320
677.581565	60441.744352	32.581338
678.602804	60532.887588	32.586356
679.010172	60639.849547	32.591373
679.731788	60731.675128	32.596391
680.205769	60817.001140	32.601408
680.859092	60937.505082	32.606426
681.880971	61032.518147	32.611444
682.232496	61121.588008	32.616461
682.779222	61244.234831	32.621479
683.585386	61339.815831	32.626496
683.974619	61464.506032	32.631514
685.163414	61557.977227	32.636532
686.035963	61670.890706	32.641549
686.630741	61784.988285	32.646567
687.398563	61879.585925	32.651584
687.880248	61988.198583	32.656602
688.646166	62101.549192	32.661620
689.015196	62209.777152	32.666637
689.867224	62326.584545	32.671655
691.001714	62428.398697	32.676672
691.822240	62533.842456	32.681690
692.555866	62646.171237	32.686708
693.418223	62742.874570	32.691725
693.998863	62845.281576	32.696743
694.876563	62947.905493	32.701760
695.274044	63057.264599	32.706778
695.972375	63160.140418	32.711796
696.350073	63263.594303	32.716813
697.200845	63376.122651	32.721831
698.282467	63480.106073	32.726848
699.101451	63589.069749	32.731866
699.462496	63694.380484	32.736884
700.489284	63801.048201	32.741901
700.860163	63904.601259	32.746919
701.547284	64008.481857	32.751936
702.040026	64128.772058	32.756954
702.881746	64226.067319	32.761972
703.977824	64336.885434	32.766989
704.232696	64454.094355	32.772007
705.074212	64558.767623	32.777024
706.283564	64660.270805	32.782042
706.797277	64767.394883	32.787060
707.524988	64874.541067	32.792077
707.909610	64985.657154	32.797095
708.971532	65093.811211	32.802112
709.348834	65202.887987	32.807130
709.621351	65325.421269	32.812148
710.549391	65431.216154	32.817165
711.121010	65541.147582	32.822183
711.953563	65665.707981	32.827200
712.528983	65782.384774	32.832218
713.314147	65902.017543	32.837236
714.079724	66027.141126	32.842253
714.596143	66138.380706	32.847271
715.288020	66235.634330	32.852288
716.223728	66373.203959	32.857306
716.915525	66485.010645	32.862324
717.995797	66597.822110	32.867341
718.340226	66720.054644	32.872359
719.208684	66827.446869	32.877376
719.919266	66946.061234	32.882394
720.853816	67056.990136	32.887412
721.360721	67172.908490	32.892429
721.900450	67284.118735	32.897447
722.774087	67398.757697	32.902464
723.671329	67522.661080	32.907482
724.212487	67627.393120	32.912500
725.292403	67742.587830	32.917517
725.970625	67840.097748	32.922535
726.627173	67940.810571	32.927552
727.222864	68056.346169	32.932570
727.783168	68164.776055	32.937588
728.754205	68261.196458	32.942605
729.303246	68373.081080	32.947623
729.870605	68474.519259	32.952640
730.536396	68593.460140	32.957658
731.144976	68703.591796	32.962676
732.235656	68808.801656	32.967693
732.489769	68937.504309	32.972711
732.963089	69052.939150	32.977728
734.160909	69182.347279	32.982746
734.793577	69295.424222	32.987764
735.472549	69412.856526	32.992781
736.081348	69543.679183	32.997799
736.874047	69650.485108	33.002816
737.752706	69788.415344	33.007834
738.377496	69919.060655	33.012852
739.380259	70040.261748	33.017869
739.962984	70148.925746	33.022887
740.770314	70271.892814	33.027904
741.627371	70398.361435	33.032922
742.167252	70526.444881	33.037940
743.089232	70642.851220	33.042957
743.806927	70763.686224	33.047975
744.937207	70890.599506	33.052992
745.568148	71017.741428	33.058010
745.822070	71134.918350	33.063028
746.866275	71260.229404	33.068045
747.820421	71398.612878	33.073063
748.274195	71518.262776	33.078080
749.413285	71636.206783	33.083098
749.620621	71763.246055	33.088116
750.228639	71891.339095	33.093133
751.037395	72029.219524	33.098151
752.006562	72153.220357	33.103168
752.841986	72289.169500	33.108186
753.308080	72416.460780	33.113204
754.567873	72540.839518	33.118221
755.040908	72658.102413	33.123239
755.765465	72793.149855	33.128256
756.954844	72943.638928	33.133274
757.570922	73062.613009	33.138292
758.343838	73176.332366	33.143309
759.176794	73313.192644	33.148327
759.855294	73427.668765	33.153344
761.266331	73549.100574	33.158362
761.921199	73676.159452	33.163380
763.006700	73797.728623	33.168397
763.571666	73908.925115	33.173415
764.158247	74020.068019	33.178432
764.734994	74143.550690	33.183450
765.610636	74277.172280	33.188468
766.301702	74383.392559	33.193485
766.657984	74513.503131	33.198503
767.395558	74652.797012	33.203520
768.437363	74765.626600	33.208538
768.954049	74895.036312	33.213556
770.312542	75025.850835	33.218573
770.985836	75149.576241	33.223591
771.283918	75265.794426	33.228608
772.358139	75406.801951	33.233626
773.175700	75523.675646	33.238644
774.172718	75637.592251	33.243661
774.364163	75777.236469	33.248679
775.441865	75900.342824	33.253696
776.136987	76013.470117	33.258714
776.764415	76134.286869	33.263732
777.808614	76249.198108	33.268749
778.431504	76374.817101	33.273767
779.101153	76488.096513	33.278784
779.854173	76604.404793	33.283802
780.460952	76727.201443	33.288820
781.136912	76846.799806	33.293837
781.952544	76981.738059	33.298855
782.936203	77108.851188	33.303872
783.809498	77220.709340	33.308890
784.759218	77363.280568	33.313908
785.367771	77492.317299	33.318925
786.041484	77614.152813	33.323943
786.910839	77737.297543	33.328960
787.275804	77870.607968	33.333978
788.188289	77997.339508	33.338996
789.137673	78124.034057	33.344013
789.507944	78267.345612	33.349031
790.660092	78398.119437	33.354048
791.488421	78532.413596	33.359066
792.269438	78663.465320	33.364084
792.994564	78795.292377	33.369101
793.825739	78931.707375	33.374119
794.411251	79067.101152	33.379136
795.474183	79206.553582	33.384154
795.818104	79345.897905	33.389172
796.991556	79483.657637	33.394189
798.045273	79621.311486	33.399207
798.561488	79759.377531	33.404224
799.398307	79898.511079	33.409242
800.060224	80043.689840	33.414260
801.148661	80172.454148	33.419277
801.756209	80312.899545	33.424295
802.510063	80462.828933	33.429312
803.304674	80598.621268	33.434330
803.823302	80741.797700	33.439348
804.973284	80883.074308	33.444365
805.837739	81033.533246	33.449383
806.797510	81166.866351	33.454400
807.360150	81306.218367	33.459418
808.183262	81457.540942	33.464436
809.043015	81586.218269	33.469453
810.083121	81737.652386	33.474471
810.826770	81880.748288	33.479488
811.768543	82024.407021	33.484506
812.698101	82174.799556	33.489524
813.663745	82305.152534	33.494541
814.437077	82448.190185	33.499559
815.201244	82584.840865	33.504576
816.371602	82720.147410	33.509594
816.693870	82855.512561	33.514612
817.791357	82985.898286	33.519629
818.565327	83127.042233	33.524647
819.401826	83270.283393	33.529664
819.967943	83402.682445	33.534682
820.695219	83547.417419	33.539700
821.593537	83689.999387	33.544717
822.417956	83839.066426	33.549735
822.895959	83982.023288	33.554752
823.762434	84125.897512	33.559770
824.809435	84273.779197	33.564788
825.732214	84423.105839	33.569805
826.277359	84554.534387	33.574823
827.305134	84710.007735	33.579840
828.316075	84838.893580	33.584858
829.224160	84989.675155	33.589876
829.910982	85119.058963	33.594893
830.939098	85260.186739	33.599911
831.207497	85392.171914	33.604928
832.060183	85516.291890	33.609946
833.158596	85654.025558	33.614964
834.014196	85787.295311	33.619981
834.740817	85925.756324	33.624999
835.343813	86070.356868	33.630016
836.443954	86204.948969	33.635034
836.686782	86350.363656	33.640052
837.826290	86484.008130	33.645069
838.593331	86630.603453	33.650087
838.789976	86773.687336	33.655104
840.094592	86927.124131	33.660122
840.733849	87083.841809	33.665140
841.547589	87236.349316	33.670157
842.577164	87389.341032	33.675175
843.465292	87539.231330	33.680192
844.166363	87695.474672	33.685210
844.772579	87850.570446	33.690228
846.149077	87992.106550	33.695245
846.543845	88160.046364	33.700263
847.315774	88316.225196	33.705280
848.478245	88469.961352	33.710298
849.301294	88631.683264	33.715316
850.171703	88790.683832	33.720333
851.251306	88949.587653	33.725351
851.829576	89107.227481	33.730368
852.803555	89262.626209	33.735386
853.860650	89422.308941	33.740404
854.705568	89582.932694	33.745421
855.444220	89735.158746	33.750439
856.103709	89896.207582	33.755456
857.308875	90067.222859	33.760474
857.972860	90222.033599	33.765492
858.789466	90383.819186	33.770509
859.755304	90549.941425	33.775527
860.470829	90716.321318	33.780544
861.511453	90868.011159	33.785562
862.264611	91038.082854	33.790580
862.919822	91208.228890	33.795597
864.496361	91360.440907	33.800615
865.055243	91536.395766	33.805632
865.939604	91686.673698	33.810650
866.954530	91851.619770	33.815668
867.614295	92023.720069	33.820685
868.317768	92182.043081	33.825703
869.630037	92355.234145	33.830720
870.415065	92516.134357	33.835738
871.267980	92678.024394	33.840756
871.755833	92837.596130	33.845773
873.163447	92989.137532	33.850791
874.036482	93159.457618	33.855808
875.124390	93322.566314	33.860826
875.898898	93486.784811	33.865844
876.520438	93644.858799	33.870861
877.601300	93797.902257	33.875879
878.150073	93967.047377	33.880896
879.465299	94131.079689	33.885914
880.395715	94289.898030	33.890932
881.315828	94468.023524	33.895949
882.014122	94618.179521	33.900967
883.026467	94769.487174	33.905984
884.105917	94935.089215	33.911002
885.432929	95091.448437	33.916020
885.753163	95250.614300	33.921037
886.840579	95394.393956	33.926055
887.533618	95553.354651	33.931072
888.821124	95701.052740	33.936090
889.317696	95851.281257	33.941108
890.142647	95999.095489	33.946125
891.186321	96139.588953	33.951143
891.984424	96299.467600	33.956160
892.657065	96435.802044	33.961178
893.660452	96591.812818	33.966196
893.933157	96735.449988	33.971213
894.995500	96891.807397	33.976231
895.657181	97056.239378	33.981248
896.492340	97221.042600	33.986266
897.862710	97374.351766	33.991284
898.497987	97545.608835	33.996301
899.527184	97707.325806	34.001319
900.343328	97872.503641	34.006336
901.277383	98026.895377	34.011354
902.265876	98195.376600	34.016372
902.974850	98367.044950	34.021389
904.014722	98519.453535	34.026407
904.982928	98688.625116	34.031424
906.063105	98852.651695	34.036442
906.868674	99023.561612	34.041460
907.422878	99193.324057	34.046477
908.591734	99355.674358	34.051495
909.225939	99534.086117	34.056512
910.211446	99704.287251	34.061530
911.300550	99881.315918	34.066548
911.907717	100058.684961	34.071565
912.696654	100232.068495	34.076583
913.407681	100417.792215	34.081600
914.421947	100589.862171	34.086618
915.315722	100778.154022	34.091636
916.103939	100963.406841	34.096653
917.498304	101140.311619	34.101671
918.112905	101337.903331	34.106688
919.056589	101517.746788	34.111706
920.151836	101699.687427	34.116724
921.017018	101888.524040	34.121741
922.044456	102055.156908	34.126759
922.990529	102247.863874	34.131776
923.731429	102435.813344	34.136794
924.672107	102614.734314	34.141812
925.555515	102818.833413	34.146829
926.797094	102992.502902	34.151847
927.650103	103189.018525	34.156864
928.649971	103364.769186	34.161882
929.630592	103559.905282	34.166900
930.385241	103735.420365	34.171917
931.488218	103924.631583	34.176935
932.494158	104113.923523	34.181952
933.253953	104304.929081	34.186970
934.363138	104489.419882	34.191988
935.165991	104681.301227	34.197005
936.176006	104857.801183	34.202023
937.011307	105060.298615	34.207040
937.402193	105248.839223	34.212058
938.411979	105432.048721	34.217076
939.292484	105644.129974	34.222093
940.344769	105827.867128	34.227111
941.408149	106031.144944	34.232128
942.213815	106233.909646	34.237146
943.140827	106420.166545	34.242164
943.903505	106632.807159	34.247181
945.383688	106825.535923	34.252199
946.353703	107013.816292	34.257216
947.294628	107206.472230	34.262234
948.473721	107391.427875	34.267252
949.191533	107590.582639	34.272269
950.511374	107772.579389	34.277287
951.244013	107958.511937	34.282304
952.106725	108136.546409	34.287322
953.057066	108319.405835	34.292340
954.062774	108492.036230	34.297357
955.290803	108670.001291	34.302375
955.705943	108853.573362	34.307392
956.727650	109038.655114	34.312410
957.592028	109224.004774	34.317428
958.649702	109425.536340	34.322445
959.403067	109604.523274	34.327463
960.527144	109796.445736	34.332480
961.295864	109993.583428	34.337498
962.482955	110178.227747	34.342516
962.872560	110373.809512	34.347533
964.010172	110566.368550	34.352551
964.920647	110757.522460	34.357568
965.997399	110964.091055	34.362586
967.225350	111155.246025	34.367604
968.199545	111357.160477	34.372621
969.081022	111552.656878	34.377639
969.940344	111758.380720	34.382656
970.587498	111967.282619	34.387674
972.279148	112149.412285	34.392692
972.670179	112365.427880	34.397709
973.412040	112564.691471	34.402727
974.800812	112767.916009	34.407744
975.516028	112998.501492	34.412762
976.385664	113200.776189	34.417780
977.463499	113415.305865	34.422797
978.361003	113629.778307	34.427815
979.358753	113857.588047	34.432832
980.377551	114062.745436	34.437850
981.515257	114269.417578	34.442868
982.193922	114500.794409	34.447885
983.023757	114718.744932	34.452903
984.229923	114931.656273	34.457920
985.386710	115160.501948	34.462938
986.415671	115368.783803	34.467956
987.241249	115598.359194	34.472973
988.394352	115819.584200	34.477991
989.584660	116035.407774	34.483008
990.539811	116262.002641	34.488026
992.204803	116456.948272	34.493044
993.035143	116671.657918	34.498061
994.096513	116887.015210	34.503079
995.598857	117098.703183	34.508096
996.247863	117308.202403	34.513114
997.735361	117507.428936	34.518132
998.454021	117707.227244	34.523149
999.892694	117897.405637	34.528167
1001.013445	118098.546677	34.533184
1002.025432	118299.656414	34.538202
1003.070729	118502.472547	34.543220
1003.963911	118700.715919	34.548237
1004.828882	118891.312416	34.553255
1006.474919	119098.848345	34.558272
1006.946199	119301.954967	34.563290
1007.742334	119487.169133	34.568308
1008.366691	119699.997015	34.573325
1009.672097	119896.900852	34.578343
1010.711377	120105.228440	34.583360
1011.491276	120309.938435	34.588378
1012.180628	120508.988179	34.593396
1013.008021	120730.115032	34.598413
1013.897907	120937.865058	34.603431
1015.210834	121152.503308	34.608448
1015.895241	121370.072639	34.613466
1017.093376	121573.746791	34.618484
1017.838796	121795.680906	34.623501
1018.956271	121994.137918	34.628519
1020.355691	122190.243459	34.633536
1021.061355	122407.107373	34.638554
1022.271118	122608.721286	34.643572
1023.005931	122805.916402	34.648589
1023.714515	123025.521562	34.653607
1025.020830	123219.013523	34.658624
1025.441233	123440.240701	34.663642
1026.693140	123663.055711	34.668660
1027.425621	123878.912217	34.673677
1028.545141	124099.268542	34.678695
1029.606482	124321.904523	34.683712
1030.554122	124557.335146	34.688730
1031.619252	124778.909396	34.693748
1032.486345	125006.689741	34.698765
1033.783871	125232.322369	34.703783
1035.354149	125450.472496	34.708800
1036.209386	125682.125255	34.713818
1037.378776	125893.171688	34.718836
1038.590423	126131.232494	34.723853
1039.397814	126345.827065	34.728871
1040.583745	126565.404788	34.733888
1041.612206	126791.359655	34.738906
1042.882632	127002.067631	34.743924
1043.661796	127247.990357	34.748941
1044.591956	127472.889232	34.753959
1046.064435	127700.843424	34.758976
1046.649382	127935.295630	34.763994
1048.179760	128159.606177	34.769012
1049.097703	128382.992841	34.774029
1049.929012	128615.952021	34.779047
1051.338032	128842.683078	34.784064
1051.992825	129089.997302	34.789082
1053.147156	129318.358239	34.794100
1054.055971	129549.765346	34.799117
1055.062478	129790.753030	34.804135
1056.317676	130025.199203	34.809152
1057.547367	130249.257695	34.814170
1058.462336	130493.384031	34.819188
1059.327617	130733.806590	34.824205
1060.292296	130967.902196	34.829223
1061.621689	131216.528936	34.834240
1062.062734	131468.257729	34.839258
1063.812173	131706.209456	34.844276
1064.519992	131947.060246	34.849293
1065.341286	132201.926446	34.854311
1066.705973	132438.578203	34.859328
1068.186402	132701.160748	34.864346
1068.983386	132928.263306	34.869364
1070.188965	133179.790767	34.874381
1071.315152	133425.413409	34.879399
1072.529543	133646.760446	34.884416
1073.337584	133895.849214	34.889434
1074.906610	134144.091719	34.894452
1076.066980	134388.803379	34.899469
1076.731591	134638.137085	34.904487
1078.469209	134859.583583	34.909504
1079.185375	135106.617853	34.914522
1079.979301	135335.563453	34.919540
1081.683401	135566.021144	34.924557
1082.699118	135810.627992	34.929575
1083.857017	136041.838447	34.934592
1084.687947	136278.112163	34.939610
1085.905613	136511.775532	34.944628
1086.676002	136751.954709	34.949645
1087.775735	137001.006492	34.954663
1088.930679	137223.592155	34.959680
1089.513818	137477.068677	34.964698
1090.680393	137703.814061	34.969716
1091.640774	137931.913574	34.974733
1092.572520	138174.421946	34.979751
1094.127326	138401.894077	34.984768
1094.635712	138638.263304	34.989786
1095.882030	138886.303474	34.994804
1096.991524	139111.445029	34.999821
1097.799566	139360.359822	35.004839
1099.106399	139607.736055	35.009856
1100.263749	139846.491743	35.014874
1101.331833	140101.746613	35.019892
1102.290876	140352.304775	35.024909
1103.342117	140596.002790	35.029927
1104.563026	140850.616805	35.034944
1105.520803	141101.041242	35.039962
1106.621890	141349.237629	35.044980
1108.012336	141602.155589	35.049997
1108.916712	141870.967246	35.055015
1109.937155	142112.259372	35.060032
1110.936515	142371.853749	35.065050
1111.892123	142648.841570	35.070068
1112.828506	142905.901691	35.075085
1114.153387	143176.340586	35.080103
1115.436096	143446.205262	35.085120
1116.405925	143709.327002	35.090138
1117.470251	143978.661246	35.095156
1118.700743	144250.430173	35.100173
1119.227883	144534.440043	35.105191
1120.738021	144805.938870	35.110208
1121.723920	145088.140227	35.115226
1122.690197	145369.243840	35.120244
1123.786683	145644.380772	35.125261
1124.763734	145933.197187	35.130279
1126.272626	146216.957100	35.135296
1127.514766	146509.107662	35.140314
1128.396656	146789.627755	35.145332
1129.874948	147066.158355	35.150349
1131.292960	147354.127236	35.155367
1132.467455	147629.647068	35.160384
1133.582712	147918.152352	35.165402
1134.642447	148198.666775	35.170420
1136.120781	148472.823963	35.175437
1137.348336	148768.254585	35.180455
1138.174299	149041.001887	35.185472
1139.309425	149312.647560	35.190490
1140.161434	149603.784207	35.195508
1141.747026	149881.307822	35.200525
1142.711939	150176.831230	35.205543
1143.963818	150446.665087	35.210560
1144.929459	150734.684650	35.215578
1145.831902	151029.870074	35.220596
1147.142599	151312.484958	35.225613
1148.290094	151609.524310	35.230631
1149.444128	151901.250661	35.235648
1150.443969	152187.157712	35.240666
1151.239806	152481.661944	35.245684
1152.563941	152779.340949	35.250701
1153.803031	153075.438201	35.255719
1155.056035	153364.610146	35.260736
1156.195236	153661.147027	35.265754
1157.334567	153955.973865	35.270772
1158.838745	154225.323943	35.275789
1159.883479	154534.820927	35.280807
1161.246500	154823.275458	35.285824
1163.192787	155102.782216	35.290842
1164.115506	155405.038226	35.295860
1165.448263	155669.276839	35.300877
1166.866580	155935.329713	35.305895
1167.995077	156188.785619	35.310912
1169.020849	156452.889963	35.315930
1170.154913	156707.578743	35.320948
1171.672868	156975.220553	35.325965
1172.663340	157234.122484	35.330983
1173.939863	157496.036010	35.336000
1175.088240	157758.264187	35.341018
1175.772548	158018.642541	35.346036
1177.281909	158286.142440	35.351053
1178.104319	158562.814935	35.356071
1179.036367	158816.992496	35.361088
1180.209173	159110.926694	35.366106
1180.937188	159387.518989	35.371124
1182.080086	159661.393374	35.376141
1183.331318	159968.349203	35.381159
1184.278233	160243.604589	35.386176
1185.410561	160528.396529	35.391194
1186.512566	160826.845769	35.396212
1187.754100	161112.080465	35.401229
1189.088842	161425.884081	35.406247
1190.219148	161731.477658	35.411264
1191.175283	162025.341841	35.416282
1192.295883	162331.969078	35.421300
1193.444009	162623.179688	35.426317
1194.587865	162944.016726	35.431335
1195.817645	163246.369922	35.436352
1197.448566	163558.745251	35.441370
1198.261370	163872.107980	35.446388
1199.967573	164178.740931	35.451405
1200.952240	164486.053446	35.456423
1201.872150	164785.867961	35.461440
1203.619569	165097.055522	35.466458
1205.065275	165410.997604	35.471476
1206.630752	165714.048915	35.476493
1207.652053	166014.388202	35.481511
1209.324768	166310.016387	35.486528
1210.616996	166614.184917	35.491546
1211.495622	166929.804980	35.496564
1212.878240	167217.874450	35.501581
1213.823534	167523.273910	35.506599
1215.199530	167834.352191	35.511616
1216.511459	168121.132388	35.516634
1217.287987	168436.247259	35.521652
1218.746844	168735.987467	35.526669
1219.804717	169043.180655	35.531687
1220.909285	169363.780205	35.536704
1222.461701	169679.219934	35.541722
1223.199813	169983.883863	35.546740
1224.725456	170296.007865	35.551757
1225.567703	170609.997916	35.556775
1227.014816	170919.309531	35.561792
1228.275469	171242.726375	35.566810
1228.901993	171565.463443	35.571828
1230.400522	171870.344458	35.576845
1231.236983	172208.913154	35.581863
1232.867628	172532.950579	35.586880
1234.414348	172848.184809	35.591898
1234.818877	173183.710275	35.596916
1236.328193	173508.675511	35.601933
1237.664254	173842.592626	35.606951
1238.831584	174166.667128	35.611968
1239.833423	174505.720124	35.616986
1240.822724	174834.930022	35.622004
1242.490849	175178.268667	35.627021
1243.535728	175503.235457	35.632039
1244.840239	175831.575335	35.637056
1246.417636	176162.550123	35.642074
1247.725147	176485.462410	35.647092
1248.847626	176791.021104	35.652109
1250.278409	177106.201221	35.657127
1251.401187	177409.771292	35.662144
1252.312029	177720.218652	35.667162
1253.498137	178045.420294	35.672180
1254.741706	178366.248847	35.677197
1255.999070	178692.800937	35.682215
1257.475805	179036.541049	35.687232
1258.850426	179343.305013	35.692250
1259.953164	179675.942839	35.697268
1261.172316	180000.859884	35.702285
1262.901690	180323.841829	35.707303
1263.860803	180665.178247	35.712320
1265.316186	180975.923987	35.717338
1266.388099	181312.220167	35.722356
1267.797328	181639.438899	35.727373
1268.909069	181969.564513	35.732391
1270.061371	182306.501198	35.737408
1271.703784	182637.888839	35.742426
1272.977593	182985.027067	35.747444
1273.933927	183327.676126	35.752461
1275.210148	183649.890561	35.757479
1276.239066	183990.881924	35.762496
1277.847497	184333.632945	35.767514
1278.618386	184687.148172	35.772532
1279.870648	185031.180939	35.777549
1281.482840	185388.077813	35.782567
1282.484007	185735.938977	35.787584
1284.182738	186086.340073	35.792602
1285.389797	186444.833904	35.797620
1286.806664	186788.520592	35.802637
1287.854414	187144.697034	35.807655
1289.005963	187496.136712	35.812672
1290.996739	187843.924019	35.817690
1292.056013	188205.246168	35.822708
1293.614687	188557.298065	35.827725
1295.108924	188897.138804	35.832743
1296.516828	189247.163498	35.837760
1297.841942	189598.866891	35.842778
1298.908368	189939.990355	35.847796
1300.224541	190291.407497	35.852813
1301.735348	190645.028797	35.857831
1302.830193	190996.372485	35.862848
1304.172501	191350.787514	35.867866
1305.138286	191707.742202	35.872884
1306.672306	192059.667162	35.877901
1308.017671	192423.139176	35.882919
1308.954147	192805.329097	35.887936
1310.464020	193150.485604	35.892954
1311.460901	193530.842137	35.897972
1312.778192	193882.204196	35.902989
1314.414659	194247.467180	35.908007
1315.648966	194618.701826	35.913024
1317.023637	194977.918810	35.918042
1318.034279	195351.898787	35.923060
1319.545655	195718.536765	35.928077
1320.814348	196088.530376	35.933095
1321.835798	196454.948813	35.938112
1323.365842	196824.649684	35.943130
1324.765399	197199.439691	35.948148
1326.110900	197563.068794	35.953165
1328.022265	197937.613585	35.958183
1329.455377	198294.770304	35.963200
1331.328083	198653.887732	35.968218
1332.318794	199004.760795	35.973236
1333.423138	199367.284417	35.978253
1335.110197	199715.786461	35.983271
1336.222110	200067.762362	35.988288
1337.303462	200404.852724	35.993306
1338.480912	200758.535371	35.998324
1339.435759	201096.919653	36.003341
1340.916480	201448.562527	36.008359
1341.983900	201804.211250	36.013376
1343.472129	202150.473239	36.018394
1344.791083	202515.606338	36.023412
1346.253425	202863.336214	36.028429
1347.711978	203220.006783	36.033447
1348.955177	203590.719022	36.038464
1350.394336	203923.653691	36.043482
1351.574547	204295.090980	36.048500
1352.836262	204662.618811	36.053517
1354.402011	205021.629526	36.058535
1355.657254	205396.551677	36.063552
1357.160524	205760.832830	36.068570
1358.432075	206128.823451	36.073588
1359.694787	206498.480660	36.078605
1361.030801	206883.541934	36.083623
1362.102917	207252.561334	36.088640
1363.333340	207626.432147	36.093658
1364.965828	208015.145105	36.098676
1365.975882	208395.315799	36.103693
1367.355810	208784.366321	36.108711
1368.780876	209171.735243	36.113728
1370.230639	209550.505712	36.118746
1371.685903	209934.521200	36.123764
1372.792085	210329.732028	36.128781
1374.400940	210731.261506	36.133799
1375.526363	211134.523457	36.138816
1377.201254	211525.887652	36.143834
1378.327810	211929.521529	36.148852
1379.626128	212324.748310	36.153869
1381.125667	212730.051407	36.158887
1382.371005	213138.801486	36.163904
1383.990473	213540.076016	36.168922
1385.592439	213935.717267	36.173940
1387.113938	214340.313205	36.178957
1388.580836	214739.789867	36.183975
1389.776864	215151.376539	36.188992
1390.952737	215563.349380	36.194010
1392.554517	215960.828257	36.199028
1393.606770	216372.139441	36.204045
1395.397912	216781.349533	36.209063
1396.335173	217195.858017	36.214080
1397.988727	217609.005643	36.219098
1399.474409	218028.303609	36.224116
1400.478798	218441.181008	36.229133
1402.190167	218865.575726	36.234151
1403.163412	219293.472032	36.239168
1404.892945	219775.063969	36.244186
1406.183532	220194.987580	36.249204
1407.488245	220615.494769	36.254221
1409.011637	221033.986527	36.259239
1410.193701	221460.130473	36.264256
1411.335408	221888.136923	36.269274
1412.807468	222319.900407	36.274292
1414.408893	222751.999877	36.279309
1415.924686	223165.675582	36.284327
1417.421423	223603.078704	36.289344
1419.241329	224028.822826	36.294362
1420.502695	224450.393676	36.299380
1421.837639	224891.003456	36.304397
1423.460357	225304.567859	36.309415
1424.937862	225736.419958	36.314432
1426.488962	226165.365952	36.319450
1427.903413	226572.238313	36.324468
1429.233298	226980.294401	36.329485
1430.686375	227374.818806	36.334503
1432.280698	227783.265742	36.339520
1433.639028	228188.933562	36.344538
1434.876157	228588.958467	36.349556
1436.144286	228990.681326	36.354573
1437.620008	229391.050365	36.359591
1439.102452	229819.004302	36.364608
1440.574563	230224.532747	36.369626
1442.320487	230641.701467	36.374644
1443.080841	231047.654644	36.379661
1444.727030	231474.545382	36.384679
1446.051845	231904.030529	36.389696
1447.595370	232321.517101	36.394714
1449.036304	232740.444263	36.399732
1450.251152	233188.341626	36.404749
1451.789110	233604.740538	36.409767
1453.505307	234036.936074	36.414784
1455.095244	234466.715150	36.419802
1456.796287	234886.138772	36.424820
1457.485306	235326.051554	36.429837
1459.196539	235761.554824	36.434855
1460.427176	236193.709361	36.439872
1461.648588	236641.793288	36.444890
1463.347855	237089.393118	36.449908
1464.802145	237525.781600	36.454925
1466.953810	237974.985554	36.459943
1468.427368	238406.368878	36.464960
1469.621810	238853.294390	36.469978
1471.427257	239295.547804	36.474996
1472.576210	239728.791274	36.480013
1474.214552	240179.964970	36.485031
1475.467632	240627.443756	36.490048
1476.520153	241090.756736	36.495066
1477.758185	241528.409342	36.500084
1479.598937	242002.491786	36.505101
1481.245893	242459.689319	36.510119
1482.573615	242917.804140	36.515136
1483.842221	243382.432638	36.520154
1485.682905	243836.400239	36.525172
1487.190128	244321.871981	36.530189
1488.764957	244768.797880	36.535207
1490.387274	245226.843046	36.540224
1491.864003	245701.119894	36.545242
1493.531924	246152.198798	36.550260
1494.729019	246630.587804	36.555277
1496.288803	247100.026793	36.560295
1497.524491	247564.566451	36.565312
1498.748117	248039.269917	36.570330
1500.389756	248503.032684	36.575348
1501.939282	248977.099459	36.580365
1504.052199	249448.965472	36.585383
1504.991108	249924.658439	36.590400
1506.503214	250399.444525	36.595418
1508.029135	250871.180536	36.600436
1509.683157	251352.015634	36.605453
1511.351721	251833.001279	36.610471
1513.160578	252305.632062	36.615488
1514.591160	252781.551916	36.620506
1516.293722	253252.270492	36.625524
1517.467514	253727.776306	36.630541
1519.309777	254206.906469	36.635559
1520.707387	254673.815219	36.640576
1522.065893	255147.894448	36.645594
1523.926918	255609.722916	36.650612
1525.630770	256095.507438	36.655629
1527.297945	256558.003491	36.660647
1528.233468	257032.305988	36.665664
1529.625505	257489.995825	36.670682
1531.327900	257934.780553	36.675700
1532.239996	258413.304372	36.680717
1534.194595	258857.260235	36.685735
1535.609763	259323.050420	36.690752
1537.013255	259784.727269	36.695770
1539.050078	260248.585960	36.700788
1540.023295	260710.079842	36.705805
1541.727074	261172.316889	36.710823
1543.234427	261634.840354	36.715840
1544.944988	262100.937508	36.720858
1546.738766	262570.958367	36.725876
1547.716162	263039.233984	36.730893
1549.082533	263514.532809	36.735911
1550.608853	263994.479288	36.740928
1552.019720	264487.730536	36.745946
1553.496739	264971.292004	36.750964
1554.587390	265470.616177	36.755981
1556.491524	265956.926400	36.760999
1558.346976	266444.539913	36.766016
1559.453948	266964.589442	36.771034
1561.473920	267462.234739	36.776052
1562.815282	267962.328683	36.781069
1564.428343	268466.594269	36.786087
1566.230798	268954.493931	36.791104
1567.527224	269472.147389	36.796122
1569.455842	269979.026683	36.801140
1570.819693	270493.416256	36.806157
1572.211749	271000.687706	36.811175
1573.666105	271506.805094	36.816192
1575.265248	272017.165603	36.821210
1577.150783	272536.928003	36.826228
1578.899500	273053.867077	36.831245
1580.120146	273582.933393	36.836263
1581.817544	274107.246058	36.841280
1582.905836	274643.622992	36.846298
1584.609656	275161.124822	36.851316
1585.978601	275694.710000	36.856333
1587.366609	276240.179383	36.861351
1589.038464	276787.455182	36.866368
1590.324552	277331.338717	36.871386
1591.907465	277878.296565	36.876404
1593.348893	278436.885363	36.881421
1594.878342	278986.745305	36.886439
1596.548612	279548.240268	36.891456
1598.297020	280096.029131	36.896474
1600.056082	280659.818114	36.901492
1601.691658	281221.898581	36.906509
1603.215323	281784.224540	36.911527
1605.086856	282344.179903	36.916544
1606.486543	282901.798286	36.921562
1608.425998	283463.110772	36.926580
1609.842259	284029.334131	36.931597
1611.618839	284586.910490	36.936615
1613.668240	285141.087027	36.941632
1615.433398	285712.886363	36.946650
1617.222020	286252.394807	36.951668
1618.598835	286809.750204	36.956685
1620.190778	287365.010632	36.961703
1622.226103	287906.072936	36.966720
1623.504308	288465.953274	36.971738
1625.468149	289016.574066	36.976756
1627.473877	289564.290162	36.981773
1628.730744	290127.114053	36.986791
1630.697503	290662.919396	36.991808
1632.020747	291216.482089	36.996826
1634.011374	291764.852321	37.001844
1635.663506	292300.855415	37.006861
1637.132298	292830.257108	37.011879
1638.932466	293344.234930	37.016896
1640.159371	293874.815144	37.021914
1642.167794	294397.237804	37.026932
1643.474273	294919.139029	37.031949
1644.847539	295457.003270	37.036967
1646.542454	295980.080309	37.041984
1647.782881	296522.812841	37.047002
1649.601963	297060.926263	37.052020
1651.122713	297600.610271	37.057037
1653.011045	298131.569959	37.062055
1655.063795	298665.852581	37.067072
1656.351617	299220.806291	37.072090
1658.470253	299750.323059	37.077108
1659.893487	300297.603784	37.082125
1661.445614	300842.930069	37.087143
1663.058340	301379.989031	37.092160
1664.710373	301941.547722	37.097178
1666.211069	302486.771965	37.102196
1668.036104	303057.007214	37.107213
1669.232991	303619.926630	37.112231
1670.834940	304172.159762	37.117248
1672.533276	304755.307626	37.122266
1674.256836	305313.914047	37.127284
1676.093818	305899.596898	37.132301
1677.516009	306465.560284	37.137319
1679.319858	307039.330068	37.142336
1680.815910	307618.988081	37.147354
1682.784361	308197.751616	37.152372
1684.549764	308782.004916	37.157389
1686.043611	309367.238646	37.162407
1688.209360	309956.090621	37.167424
1689.727220	310540.880423	37.172442
1691.400299	311118.250381	37.177460
1692.599685	311703.770050	37.182477
1694.292133	312299.819213	37.187495
1696.399104	312891.402192	37.192512
1698.129240	313487.664689	37.197530
1699.858452	314075.771124	37.202548
1701.696627	314680.894599	37.207565
1703.223357	315276.084754	37.212583
1705.280148	315868.821099	37.217600
1706.760530	316480.286713	37.222618
1708.332074	317068.624166	37.227636
1709.984700	317672.128605	37.232653
1711.900988	318270.226540	37.237671
1714.090064	318860.961304	37.242688
1715.931179	319479.121684	37.247706
1717.524539	320071.671172	37.252724
1718.967739	320671.654823	37.257741
1720.935164	321290.565231	37.262759
1722.713529	321876.923639	37.267776
1724.265749	322491.143217	37.272794
1725.792774	323087.206531	37.277812
1727.211179	323691.128144	37.282829
1728.981575	324310.220494	37.287847
1730.946927	324922.190764	37.292864
1732.531137	325536.122284	37.297882
1734.343115	326154.580438	37.302900
1736.213692	326764.847295	37.307917
1737.795485	327382.747217	37.312935
1739.711824	327993.832177	37.317952
1741.386709	328601.954913	37.322970
1743.144395	329223.437682	37.327988
1745.009027	329830.171027	37.333005
1746.294185	330458.192857	37.338023
1748.153688	331068.900197	37.343040
1749.791128	331696.596678	37.348058
1751.426737	332301.133334	37.353076
1752.803632	332911.722997	37.358093
1754.490410	333514.359641	37.363111
1756.447082	334114.888969	37.368128
1757.987255	334729.519119	37.373146
1759.575830	335341.291200	37.378164
1761.313889	335957.144256	37.383181
1763.061633	336597.434854	37.388199
1764.545751	337196.434374	37.393216
1766.490815	337830.839094	37.398234
1767.819902	338464.373207	37.403252
1769.767027	339094.243927	37.408269
1770.999517	339746.435805	37.413287
1772.988424	340381.030773	37.418304
1774.699864	341050.210229	37.423322
1776.771679	341690.791035	37.428340
1778.559685	342340.269030	37.433357
1780.160307	343001.876822	37.438375
1782.010915	343654.423966	37.443392
1783.660026	344317.732090	37.448410
1785.128454	344982.558489	37.453428
1787.730386	345645.513632	37.458445
1789.158443	346317.942527	37.463463
1791.280040	346976.669141	37.468480
1793.235329	347634.779511	37.473498
1795.117617	348300.125828	37.478516
1797.149192	348959.956127	37.483533
1799.013946	349629.372292	37.488551
1801.414955	350292.396394	37.493568
1802.984783	350958.288764	37.498586
1804.438671	351626.474427	37.503604
1806.920012	352289.354448	37.508621
1808.111474	352963.628552	37.513639
1810.104706	353627.178133	37.518656
1811.794372	354298.888089	37.523674
1813.368498	354980.224120	37.528692
1815.305355	355662.758341	37.533709
1817.200332	356342.192885	37.538727
1818.880363	357019.216104	37.543744
1820.892163	357697.214099	37.548762
1822.139877	358385.045292	37.553780
1824.236831	359083.331058	37.558797
1826.027251	359781.731734	37.563815
1827.566713	360479.451521	37.568832
1829.680807	361178.536170	37.573850
1831.172819	361877.178581	37.578868
1833.156231	362579.254387	37.583885
1835.180634	363277.809965	37.588903
1837.280379	363983.622054	37.593920
1839.219145	364684.298022	37.598938
1840.769017	365390.074082	37.603956
1842.868111	366069.540817	37.608973
1844.301765	366785.813317	37.613991
1846.334039	367495.682494	37.619008
1848.880197	368189.015643	37.624026
1850.600810	368889.803310	37.629044
1852.800231	369590.651149	37.634061
1854.274808	370280.292205	37.639079
1856.596215	370974.803145	37.644096
1858.576527	371665.653995	37.649114
1859.986316	372361.811035	37.654132
1862.105677	373051.090912	37.659149
1864.163553	373767.405356	37.664167
1865.767611	374460.268873	37.669184
1867.574723	375150.016615	37.674202
1868.960600	375862.722398	37.679220
1871.016720	376562.343515	37.684237
1872.437019	377254.193655	37.689255
1873.862351	377954.347517	37.694272
1875.802783	378647.859410	37.699290
1876.927155	379339.818245	37.704308
1879.409381	380043.457881	37.709325
1880.928021	380741.764507	37.714343
1882.581651	381443.736744	37.719360
1885.045923	382142.137400	37.724378
1886.561624	382854.372674	37.729396
1888.311987	383553.419432	37.734413
1890.022044	384280.400173	37.739431
1891.854846	385005.645817	37.744448
1893.452877	385728.809678	37.749466
1894.935216	386462.625272	37.754484
1896.989727	387206.040242	37.759501
1898.941739	387953.207161	37.764519
1900.570669	388706.798691	37.769536
1903.034469	389451.336193	37.774554
1904.808911	390219.622437	37.779572
1906.511854	390966.227008	37.784589
1908.553983	391730.477350	37.789607
1910.450524	392487.787189	37.794624
1912.580412	393241.237659	37.799642
1914.513251	394024.866244	37.804660
1916.473720	394780.968267	37.809677
1918.095706	395548.285168	37.814695
1920.541478	396322.036646	37.819712
1922.209594	397095.034669	37.824730
1924.361516	397892.035693	37.829748
1926.237481	398668.633487	37.834765
1927.773502	399440.375604	37.839783
1930.289396	400247.694341	37.844800
1932.238743	401013.776665	37.849818
1933.804649	401797.691595	37.854836
1935.703612	402595.873061	37.859853
1937.660962	403385.736493	37.864871
1939.780124	404185.560321	37.869888
1942.127538	404979.470714	37.874906
1943.746654	405773.250802	37.879924
1945.958264	406565.998534	37.884941
1947.881265	407366.980275	37.889959
1949.966253	408176.703588	37.894976
1951.626910	408971.348168	37.899994
1953.475134	409778.529823	37.905012
1955.876153	410570.117694	37.910029
1957.923183	411379.017675	37.915047
1959.491633	412180.296753	37.920064
1962.019509	412989.828899	37.925082
1963.796424	413800.397537	37.930100
1965.624164	414602.244979	37.935117
1967.690419	415423.785157	37.940135
1969.472953	416221.614077	37.945152
1971.822231	417039.738869	37.950170
1973.509255	417860.986270	37.955188
1975.402122	418668.497780	37.960205
1977.200442	419487.902159	37.965223
1979.046395	420311.425542	37.970240
1981.294916	421125.562252	37.975258
1983.066929	421964.288685	37.980276
1984.911275	422786.997369	37.985293
1986.937954	423608.762714	37.990311
1988.885576	424460.948385	37.995328
1990.994726	425275.631384	38.000346
1992.877712	426116.402398	38.005364
1994.935338	426947.950940	38.010381
1996.821951	427782.841097	38.015399
1998.802195	428608.472248	38.020416
2001.273324	429436.475043	38.025434
2003.183175	430273.148541	38.030452
2004.883529	431086.387590	38.035469
2007.147718	431887.862319	38.040487
2009.003951	432687.251057	38.045504
2011.468084	433493.852409	38.050522
2013.524380	434307.225584	38.055540
2015.422250	435084.962088	38.060557
2017.607397	435893.146283	38.065575
2019.294892	436713.025437	38.070592
2021.615624	437506.149134	38.075610
2023.326130	438324.701654	38.080628
2025.129300	439140.729709	38.085645
2027.137893	439951.684514	38.090663
2028.930447	440783.241899	38.095680
2031.134900	441601.493303	38.100698
2032.727958	442446.077448	38.105716
2034.740344	443280.491244	38.110733
2036.969166	444125.412712	38.115751
2038.656092	444976.816765	38.120768
2040.564140	445828.151354	38.125786
2042.898501	446685.605185	38.130804
2044.956136	447545.296779	38.135821
2046.838058	448403.566789	38.140839
2048.923210	449258.278747	38.145856
2051.371665	450118.460872	38.150874
2053.240039	450989.983563	38.155892
2055.371946	451857.987703	38.160909
2057.214254	452725.144189	38.165927
2059.328514	453604.964944	38.170944
2061.626481	454476.980878	38.175962
2063.318962	455377.025656	38.180980
2065.418518	456256.180772	38.185997
2067.769244	457136.369532	38.191015
2069.415544	458038.480405	38.196032
2071.587219	458924.993052	38.201050
2073.599746	459832.627236	38.206068
2075.529017	460735.532745	38.211085
2077.737053	461637.037500	38.216103
2079.537536	462554.139246	38.221120
2081.844731	463461.510858	38.226138
2083.696595	464374.981988	38.231156
2086.019533	465299.200664	38.236173
2088.590159	466225.104231	38.241191
2090.573805	467141.710904	38.246208
2092.556442	468056.101635	38.251226
2094.489056	468973.186625	38.256244
2096.649471	469899.539395	38.261261
2098.807668	470821.148648	38.266279
2100.787155	471756.941751	38.271296
2103.110265	472670.906061	38.276314
2105.111944	473607.867877	38.281332
2107.365725	474533.071352	38.286349
2109.788063	475459.616187	38.291367
2111.860201	476401.479535	38.296384
2114.109153	477324.980265	38.301402
2116.440418	478259.887688	38.306420
2118.502701	479185.498686	38.311437
2120.962373	480109.987601	38.316455
2122.940250	481041.933494	38.321472
2124.866584	481956.064003	38.326490
2127.161425	482880.591591	38.331508
2129.373656	483817.810675	38.336525
2131.284148	484745.437135	38.341543
2133.149785	485678.173206	38.346560
2135.636095	486606.668805	38.351578
2137.803043	487550.162911	38.356596
2139.549311	488485.397067	38.361613
2141.797989	489425.244043	38.366631
2144.472289	490355.581849	38.371648
2146.346858	491260.159045	38.376666
2148.145883	492160.462170	38.381684
2150.179719	493078.697618	38.386701
2152.292418	493987.635936	38.391719
2154.155721	494890.965951	38.396736
2156.246766	495807.028168	38.401754
2158.152614	496728.723279	38.406772
2160.219356	497655.841734	38.411789
2162.439184	498585.911510	38.416807
2164.526875	499523.216787	38.421824
2166.535608	500449.283507	38.426842
2168.274473	501393.201103	38.431860
2170.399283	502354.656434	38.436877
2172.440467	503312.589685	38.441895
2174.005448	504276.598410	38.446912
2176.663398	505245.666077	38.451930
2178.507300	506209.666932	38.456948
2180.941750	507197.970823	38.461965
2183.308110	508174.830148	38.466983
2185.612189	509165.809266	38.472000
2187.870805	510143.323934	38.477018
2190.419626	511138.679096	38.482036
2192.393253	512124.136176	38.487053
2194.996706	513105.698339	38.492071
2197.170853	514101.787488	38.497088
2199.246953	515080.189323	38.502106
2201.873233	516069.779581	38.507124
2203.739080	517079.389705	38.512141
2206.105440	518077.009862	38.517159
2208.175674	519082.022235	38.522176
2210.618405	520081.365622	38.527194
2213.346887	521081.756086	38.532212
2215.405388	522091.965673	38.537229
2217.923840	523092.813993	38.542247
2219.889125	524087.441670	38.547264
2222.091939	525102.465655	38.552282
2224.202343	526115.019300	38.557300
2226.232309	527129.935702	38.562317
2228.567608	528137.128945	38.567335
2230.679247	529174.051800	38.572352
2232.713647	530188.256615	38.577370
2234.659622	531208.499026	38.582388
2236.830587	532254.259953	38.587405
2239.446307	533280.944713	38.592423
2241.767438	534326.684550	38.597440
2243.732506	535373.263994	38.602458
2246.220321	536401.562758	38.607476
2248.133356	537458.972830	38.612493
2250.379161	538510.362746	38.617511
2252.139893	539560.749425	38.622528
2254.792644	540611.314601	38.627546
2257.286072	541673.551651	38.632564
2259.376489	542728.732526	38.637581
2261.792828	543786.698786	38.642599
2263.928215	544859.169205	38.647616
2266.021889	545910.741400	38.652634
2268.883025	546974.128343	38.657652
2270.862985	548051.006938	38.662669
2272.890574	549101.745946	38.667687
2275.385854	550179.581126	38.672704
2277.428441	551260.976432	38.677722
2279.572925	552325.628930	38.682740
2281.633210	553404.288201	38.687757
2283.698172	554489.194897	38.692775
2285.948338	555578.608491	38.697792
2288.538128	556659.535408	38.702810
2291.191023	557742.224573	38.707828
2293.372419	558827.115113	38.712845
2295.454607	559886.258094	38.717863
2298.134279	560940.596026	38.722880
2299.984822	562003.276183	38.727898
2302.378798	563047.546253	38.732916
2304.419681	564102.993091	38.737933
2306.784819	565157.749083	38.742951
2308.965906	566228.521414	38.747968
2311.222999	567301.252123	38.752986
2313.683330	568371.952518	38.758004
2315.814553	569449.346597	38.763021
2317.772181	570524.620762	38.768039
2320.232667	571608.256150	38.773056
2322.253970	572696.791410	38.778074
2324.842966	573793.923781	38.783092
2327.169247	574890.552930	38.788109
2329.426551	575989.105708	38.793127
2331.735185	577096.586549	38.798144
2334.060973	578209.887506	38.803162
2336.635636	579316.024443	38.808180
2338.721411	580439.150082	38.813197
2341.368889	581552.199684	38.818215
2343.708230	582691.582479	38.823232
2345.924492	583796.475698	38.828250
2348.287641	584929.729236	38.833268
2350.595402	586075.723541	38.838285
2353.317109	587200.934948	38.843303
2355.790753	588342.075624	38.848320
2357.524176	589484.133001	38.853338
2360.362498	590622.391315	38.858356
2362.600674	591778.483172	38.863373
2364.837174	592926.495368	38.868391
2366.746824	594078.409547	38.873408
2369.169957	595254.428178	38.878426
2371.575518	596429.130408	38.883444
2373.685586	597599.406030	38.888461
2376.065904	598772.175235	38.893479
2378.269474	599959.330503	38.898496
2380.454047	601159.789317	38.903514
2383.481178	602339.554776	38.908532
2385.197678	603537.941611	38.913549
2387.791733	604738.111817	38.918567
2390.547324	605939.681767	38.923584
2392.312012	607138.786189	38.928602
2395.174959	608351.847158	38.933620
2397.422210	609565.430498	38.938637
2400.217269	610764.582702	38.943655
2403.004942	611987.824078	38.948672
2405.005304	613204.408445	38.953690
2407.827287	614412.621645	38.958708
2410.174143	615625.383649	38.963725
2412.561691	616839.106739	38.968743
2415.190275	618051.106812	38.973760
2417.574809	619264.863845	38.978778
2419.889676	620485.747343	38.983796
2422.140484	621699.906775	38.988813
2424.783230	622917.365197	38.993831
2427.549606	624141.063868	38.998848
2429.631550	625367.135661	39.003866
2432.299800	626576.682656	39.008884
2434.742907	627805.315280	39.013901
2437.100466	629025.428744	39.018919
2439.647152	630245.071836	39.023936
2442.187478	631459.531854	39.028954
2444.774724	632686.928438	39.033972
2446.930649	633921.992765	39.038989
2449.417070	635129.897921	39.044007
2451.795078	636352.408060	39.049024
2454.365868	637568.454217	39.054042
2456.726748	638755.496176	39.059060
2458.950141	639958.393720	39.064077
2461.039546	641151.094308	39.069095
2463.511010	642352.973313	39.074112
2465.999817	643539.843083	39.079130
2468.478512	644754.758530	39.084148
2470.872479	645960.366568	39.089165
2473.108715	647161.269820	39.094183
2475.510134	648378.108646	39.099200
2477.754341	649600.310774	39.104218
2480.301078	650835.723944	39.109236
2482.679114	652069.916141	39.114253
2485.138833	653303.942415	39.119271
2487.727642	654542.976835	39.124288
2489.824816	655803.063035	39.129306
2492.461294	657042.175547	39.134324
2494.826869	658300.354352	39.139341
2496.951249	659562.396129	39.144359
2499.771004	660842.137846	39.149376
2501.946880	662122.116499	39.154394
2504.580012	663399.809996	39.159412
2507.120256	664686.857990	39.164429
2509.200925	665980.977283	39.169447
2512.037822	667279.475737	39.174464
2513.937203	668574.917486	39.179482
2516.929214	669883.884199	39.184500
2519.680372	671202.012850	39.189517
2521.877921	672519.502395	39.194535
2524.863047	673826.732203	39.199552
2527.453294	675158.558512	39.204570
2529.949062	676474.401311	39.209588
2532.324149	677803.251993	39.214605
2534.951630	679142.010945	39.219623
2537.444613	680467.529033	39.224640
2539.775860	681805.007898	39.229658
2542.718071	683147.656978	39.234676
2544.921650	684493.559729	39.239693
2547.096763	685852.828326	39.244711
2549.796773	687205.004558	39.249728
2552.186519	688561.300849	39.254746
2555.035546	689918.658762	39.259764
2557.914851	691282.955273	39.264781
2560.169066	692654.641901	39.269799
2563.183764	694022.569369	39.274816
2565.440647	695399.144302	39.279834
2568.404000	696754.257533	39.284852
2570.626352	698142.616253	39.289869
2572.935197	699521.320352	39.294887
2575.805892	700884.940209	39.299904
2578.710466	702276.005729	39.304922
2581.381459	703662.625664	39.309940
2584.127702	705022.597230	39.314957
2586.862218	706411.147454	39.319975
2589.659621	707791.785221	39.324992
2592.070889	709165.825934	39.330010
2594.760702	710534.648275	39.335028
2597.621293	711923.675557	39.340045
2599.934296	713290.979785	39.345063
2602.844620	714659.203426	39.350080
2605.305746	716049.652542	39.355098
2608.093928	717412.204651	39.360116
2610.906680	718785.170439	39.365133
2613.307794	720167.379111	39.370151
2615.970971	721535.169574	39.375168
2618.756660	722900.935013	39.380186
2621.471864	724267.328158	39.385204
2624.000065	725655.774304	39.390221
2626.173172	727020.615145	39.395239
2628.942022	728347.224005	39.400256
2631.492207	729702.957279	39.405274
2633.939729	731045.093367	39.410292
2636.494390	732379.136295	39.415309
2638.881821	733724.544960	39.420327
2641.188383	735069.891457	39.425344
2643.663458	736439.425888	39.430362
2645.981073	737804.211407	39.435380
2648.466015	739185.419597	39.440397
2651.037160	740565.930642	39.445415
2653.499935	741953.966533	39.450432
2655.991711	743347.970597	39.455450
2658.341803	744754.526821	39.460468
2661.180343	746154.488806	39.465485
2663.865370	747576.660252	39.470503
2666.438311	748994.451085	39.475520
2668.890754	750418.165083	39.480538
2671.168428	751855.198665	39.485556
2674.009889	753292.956916	39.490573
2676.481081	754750.212308	39.495591
2679.183320	756210.355124	39.500608
2681.828821	757680.766930	39.505626
2684.233912	759145.126480	39.510644
2687.548980	760627.758859	39.515661
2690.092499	762117.463122	39.520679
2692.947309	763577.301840	39.525696
2695.212507	765064.896580	39.530714
2697.920135	766558.665448	39.535732
2700.652742	768070.375525	39.540749
2702.934259	769592.276442	39.545767
2705.972609	771091.278757	39.550784
2709.241269	772612.250910	39.555802
2711.538721	774134.003661	39.560820
2714.468976	775654.600968	39.565837
2716.644042	777182.571023	39.570855
2719.613658	778717.456315	39.575872
2722.201324	780256.254182	39.580890
2724.946085	781786.062035	39.585908
2728.250081	783319.134811	39.590925
2731.046766	784884.001633	39.595943
2734.000262	786401.365646	39.600960
2737.011114	787949.832936	39.605978
2739.716281	789486.297105	39.610996
2742.656625	791018.910595	39.616013
2745.088301	792564.655717	39.621031
2747.858687	794110.448034	39.626048
2751.065096	795659.895142	39.631066
2753.511940	797200.016172	39.636084
2757.004284	798752.846224	39.641101
2759.191946	800306.181870	39.646119
2761.779181	801834.780323	39.651136
2764.970291	803397.144900	39.656154
2767.534210	804942.773149	39.661172
2770.492911	806486.081678	39.666189
2773.099816	808039.711722	39.671207
2776.063092	809594.836452	39.676224
2778.849456	811147.533606	39.681242
2781.468038	812699.707810	39.686260
2784.631448	814246.599664	39.691277
2787.299094	815813.829699	39.696295
2790.152542	817371.727644	39.701312
2792.801941	818919.386541	39.706330
2795.412948	820487.631612	39.711348
2798.466025	822045.870125	39.716365
2801.021375	823602.165811	39.721383
2803.211228	825174.299309	39.726400
2806.105346	826757.985742	39.731418
2808.613752	828329.166260	39.736436
2811.458227	829875.057638	39.741453
2813.930377	831416.892001	39.746471
2816.815985	832962.092380	39.751488
2819.608994	834501.484739	39.756506
2822.198442	836046.727645	39.761524
2825.044769	837583.865864	39.766541
2828.206716	839153.581168	39.771559
2830.718886	840706.231797	39.776576
2833.584916	842258.543313	39.781594
2836.398688	843825.803590	39.786612
2839.519411	845389.416546	39.791629
2842.314375	846957.459575	39.796647
2845.251574	848534.030220	39.801664
2847.775848	850108.620790	39.806682
2850.434115	851698.044336	39.811700
2853.238374	853281.696925	39.816717
2855.596776	854887.545033	39.821735
2858.844440	856491.082889	39.826752
2862.107288	858097.598028	39.831770
2864.352254	859719.287064	39.836788
2867.295222	861327.047214	39.841805
2870.127322	862962.813719	39.846823
2873.030166	864598.129175	39.851840
2875.890462	866221.478248	39.856858
2878.325236	867873.334389	39.861876
2881.521298	869509.599061	39.866893
2884.629768	871172.739956	39.871911
2887.563706	872827.703119	39.876928
2890.391190	874491.612678	39.881946
2893.441539	876157.051937	39.886964
2896.673396	877801.197258	39.891981
2899.166514	879474.983636	39.896999
2902.239031	881142.978613	39.902016
2905.554338	882811.619301	39.907034
2908.367348	884487.789322	39.912052
2911.746907	886157.878571	39.917069
2914.466578	887832.328011	39.922087
2917.779569	889511.215309	39.927104
2920.596449	891184.291740	39.932122
2923.112526	892868.411915	39.937140
2926.462470	894534.635832	39.942157
2929.040324	896223.256278	39.947175
2931.843587	897912.881264	39.952192
2935.191020	899598.926471	39.957210
2937.903437	901298.638564	39.962228
2940.564668	902978.778460	39.967245
2942.904639	904706.414326	39.972263
2946.242255	906397.453337	39.977280
2949.241846	908115.553752	39.982298
2951.635570	909842.072632	39.987316
2954.879797	911561.182916	39.992333
2957.511763	913283.415992	39.997351
2960.558817	915026.375604	40.002368
2963.545148	916759.665554	40.007386
2966.811641	918504.460633	40.012404
2969.995469	920233.158223	40.017421
2972.607525	921971.189398	40.022439
2975.398152	923712.663019	40.027456
2978.653690	925438.823625	40.032474
2981.425287	927189.535035	40.037492
2984.352117	928930.926879	40.042509
2987.281979	930687.369094	40.047527
2990.131662	932450.908113	40.052544
2993.213147	934198.119171	40.057562
2996.376956	935959.002239	40.062580
2999.284391	937700.488183	40.067597
3002.101213	939462.265549	40.072615
3005.330763	941212.767567	40.077632
3008.472514	942923.024789	40.082650
3011.272305	944642.332418	40.087668
3014.763975	946355.319496	40.092685
3017.363968	948053.846971	40.097703
3019.616548	949764.091697	40.102720
3022.942226	951486.569464	40.107738
3025.317665	953217.496629	40.112756
3028.427489	954948.066568	40.117773
3031.394921	956730.507501	40.122791
3034.024551	958511.378148	40.127808
3037.360459	960309.181316	40.132826
3040.059049	962121.189647	40.137844
3043.180720	963932.753772	40.142861
3045.865695	965761.401509	40.147879
3048.461804	967592.021276	40.152896
3052.031634	969418.188141	40.157914
3054.753271	971282.459189	40.162932
3057.368059	973122.241984	40.167949
3060.264411	974988.595972	40.172967
3062.956857	976865.878913	40.177984
3066.248561	978747.027689	40.183002
3068.848950	980648.812246	40.188020
3071.939562	982549.785528	40.193037
3075.043567	984455.672837	40.198055
3077.560886	986377.565123	40.203072
3080.834441	988309.386720	40.208090
3083.976102	990264.111114	40.213108
3086.929330	992194.568806	40.218125
3090.176842	994147.745588	40.223143
3093.176760	996124.289368	40.228160
3096.383514	998085.153018	40.233178
3099.395429	1000062.361178	40.238196
3102.502851	1002026.536781	40.243213
3105.653103	1004021.361821	40.248231
3108.788007	1006008.986923	40.253248
3111.880808	1008009.105043	40.258266
3114.688258	1009995.961265	40.263284
3117.677574	1012002.723793	40.268301
3120.674302	1014011.094249	40.273319
3124.037754	1016030.886098	40.278336
3127.160371	1018046.797811	40.283354
3130.429515	1020078.892237	40.288372
3132.893154	1022107.481751	40.293389
3136.369033	1024138.940583	40.298407
3139.269593	1026194.883759	40.303424
3142.488210	1028227.606212	40.308442
3145.659888	1030270.702527	40.313460
3148.944767	1032321.237901	40.318477
3151.740990	1034386.346732	40.323495
3154.657430	1036446.618853	40.328512
3158.164409	1038504.391814	40.333530
3161.228239	1040574.200009	40.338548
3164.646955	1042654.644946	40.343565
3167.980702	1044716.119428	40.348583
3171.192844	1046793.600901	40.353600
3173.996512	1048867.964244	40.358618
3177.189722	1050942.832793	40.363636
3180.297743	1053015.974834	40.368653
3183.848408	1055109.224161	40.373671
3186.645975	1057184.600840	40.378688
3190.005761	1059268.325915	40.383706
3193.206824	1061347.063221	40.388724
3196.317275	1063436.837194	40.393741
3199.933600	1065527.556336	40.398759
3203.216419	1067602.474521	40.403776
3206.241197	1069689.594664	40.408794
3209.406479	1071779.347171	40.413812
3212.761510	1073830.041597	40.418829
3216.061676	1075871.164538	40.423847
3219.108097	1077913.385684	40.428864
3222.308695	1079946.012375	40.433882
3225.540507	1081972.231633	40.438900
3228.456632	1084003.104623	40.443917
3231.841802	1086033.524815	40.448935
3234.819211	1088078.065937	40.453952
3237.481792	1090117.112941	40.458970
3240.628873	1092172.406623	40.463988
3243.227702	1094244.097482	40.469005
3246.547958	1096324.418660	40.474023
3249.476232	1098414.114647	40.479040
3252.738986	1100511.147007	40.484058
3256.014077	1102610.507853	40.489076
3258.982648	1104723.678070	40.494093
3262.358198	1106841.285387	40.499111
3265.139138	1108981.860593	40.504128
3268.313987	1111101.060354	40.509146
3271.590266	1113256.122699	40.514164
3274.751669	1115411.003941	40.519181
3278.357438	1117571.788607	40.524199
3280.904611	1119739.000773	40.529216
3284.584857	1121922.241739	40.534234
3287.875492	1124110.160358	40.539252
3291.044615	1126295.873714	40.544269
3294.583030	1128483.949870	40.549287
3297.605652	1130694.060655	40.554304
3301.027485	1132892.194526	40.559322
3304.142064	1135114.572954	40.564340
3307.368615	1137331.457575	40.569357
3311.091242	1139561.815097	40.574375
3314.081500	1141787.191327	40.579392
3317.507526	1144017.328680	40.584410
3321.023187	1146262.485799	40.589428
3324.086545	1148496.274410	40.594445
3327.907052	1150721.436321	40.599463
3331.237152	1152982.841901	40.604480
3334.581481	1155235.252079	40.609498
3337.905850	1157473.400178	40.614516
3340.897880	1159722.152146	40.619533
3344.817628	1161984.772550	40.624551
3347.713129	1164249.975871	40.629568
3351.583459	1166489.366821	40.634586
3354.919670	1168763.277462	40.639604
3357.840342	1171034.196482	40.644621
3361.655631	1173282.537634	40.649639
3364.829484	1175560.282939	40.654656
3368.043941	1177830.165500	40.659674
3371.649458	1180100.401312	40.664692
3374.956808	1182374.387559	40.669709
3378.863111	1184645.964433	40.674727
3381.969427	1186923.805518	40.679744
3385.249678	1189198.271452	40.684762
3388.735965	1191476.856914	40.689780
3392.032239	1193773.389902	40.694797
3395.616229	1196041.980792	40.699815
3398.850139	1198327.973810	40.704832
3402.257764	1200612.922617	40.709850
3405.360148	1202892.978565	40.714868
3408.894800	1205182.231814	40.719885
3412.345964	1207479.071666	40.724903
3415.210958	1209767.881090	40.729920
3418.930967	1212066.913154	40.734938
3421.973304	1214366.328579	40.739956
3425.114306	1216686.420269	40.744973
3428.230137	1218987.377108	40.749991
3431.887529	1221302.391826	40.755008
3435.178631	1223589.527043	40.760013
3438.952093	1225849.921775	40.765018
3442.148948	1228033.658002	40.770023
3444.957630	1230154.882437	40.775028
3448.111646	1232204.883203	40.780032
3451.402815	1234173.530982	40.785037
3454.639946	1236080.230420	40.790042
3457.318300	1237905.023696	40.795047
3460.195519	1239639.032418	40.800052
3463.032166	1241314.859831	40.805056
3465.530957	1242883.874979	40.810061
3468.472981	1244400.257729	40.815066
3470.957653	1245839.663139	40.820071
3473.342872	1247184.719982	40.825076
3475.384629	1248479.489135	40.830080
3477.883917	1249698.334185	40.835085
3480.548163	1250843.401352	40.840090
3482.344292	1251919.460426	40.845095
3484.174088	1252913.133350	40.850100
3486.092634	1253872.534239	40.855104
3487.935345	1254759.016256	40.860109
3489.808333	1255591.155668	40.865114
3491.062400	1256369.364726	40.870119
3492.846723	1257076.692079	40.875124
3494.019697	1257763.432789	40.880128
3495.431638	1258379.755859	40.885133
3497.130008	1258952.937112	40.890138
3498.138163	1259486.211402	40.895143
3499.222032	1259969.917960	40.900148
3500.650829	1260406.622055	40.905152
3501.992138	1260808.640757	40.910157
3502.839316	1261184.575177	40.915162
3504.053109	1261519.277782	40.920167
3505.116914	1261813.490557	40.925172
3505.804003	1262080.785593	40.930176
3506.678574	1262306.250292	40.935181
3507.668769	1262509.728557	40.940186
3508.427731	1262680.255657	40.945191
3509.533603	1262819.777871	40.950196
3510.275733	1262937.586058	40.955200
3511.032331	1263028.895003	40.960205
3511.839960	1263076.933067	40.965210
3512.267605	1263123.273175	40.970215
3512.874906	1263141.607653	40.975220
3513.323081	1263139.496023	40.980224
3513.876662	1263121.711727	40.985229
3514.675396	1263069.982311	40.990234
3514.753208	1263016.888890	40.995239
3515.492397	1262935.246027	41.000244
3515.962498	1262846.234931	41.005248
3516.090582	1262742.177921	41.010253
3516.603061	1262622.676492	41.015258
3517.059823	1262502.810788	41.020263
3517.579292	1262340.313229	41.025268
3517.576603	1262173.171076	41.030272
3518.314427	1262003.584969	41.035277
3518.809939	1261808.644359	41.040282
3518.698618	1261618.521879	41.045287
3518.836774	1261412.783047	41.050292
3519.108988	1261190.518234	41.055296
3519.329163	1260967.881381	41.060301
3519.711673	1260738.905658	41.065306
3519.843559	1260497.819120	41.070311
3520.382026	1260242.379942	41.075316
3520.315954	1259983.041424	41.080320
3520.449859	1259718.928872	41.085325
3520.754053	1259446.245584	41.090330
3520.626093	1259177.234191	41.095335
3520.436935	1258892.920629	41.100340
3520.814034	1258619.438441	41.105344
3521.055746	1258328.160551	41.110349
3520.952186	1258043.784513	41.115354
3521.224983	1257732.251666	41.120359
3521.357832	1257431.109420	41.125364
3521.302006	1257131.371282	41.130368
3521.247739	1256821.412164	41.135373
3521.361724	1256501.388235	41.140378
3521.510181	1256194.603375	41.145383
3521.843543	1255863.649096	41.150388
3521.661764	1255538.695407	41.155392
3521.602192	1255210.917000	41.160397
3522.285248	1254887.634209	41.165402
3522.335019	1254550.330098	41.170407
3522.710056	1254205.989621	41.175412
3522.186993	1253865.207207	41.180416
3522.289051	1253524.298619	41.185421
3522.224685	1253164.830237	41.190426
3522.333509	1252812.362334	41.195431
3522.599951	1252464.299644	41.200436
3522.472471	1252109.128983	41.205440
3522.469049	1251737.850275	41.210445
3522.569084	1251399.025582	41.215450
3522.686681	1251036.867399	41.220455
3522.943664	1250668.438042	41.225460
3522.730291	1250303.959730	41.230464
3522.363134	1249948.582444	41.235469
3522.648694	1249573.844973	41.240474
3522.509512	1249214.476856	41.245479
3522.676548	1248854.010653	41.250484
3522.653473	1248483.051392	41.255488
3522.686234	1248107.038161	41.260493
3522.761458	1247738.702171	41.265498
3522.168201	1247368.776539	41.270503
3523.027559	1246994.402363	41.275508
3522.587546	1246627.649569	41.280512
3522.855570	1246249.692554	41.285517
3522.598933	1245871.886457	41.290522
3522.419561	1245505.659466	41.295527
3522.640805	1245117.399135	41.300532
3522.660861	1244740.670989	41.305536
3522.438948	1244374.089593	41.310541
3522.589957	1243999.608909	41.315546
3522.418513	1243607.298034	41.320551
3522.827038	1243228.904670	41.325556
3522.828486	1242852.875160	41.330560
3522.852238	1242476.441797	41.335565
3522.607715	1242074.070433	41.340570
3522.521840	1241698.434150	41.345575
3522.552125	1241319.959523	41.350580
3522.418054	1240947.624565	41.355584
3522.733085	1240567.185540	41.360589
3522.717673	1240166.950327	41.365594
3522.454546	1239794.737507	41.370599
3522.553703	1239398.331197	41.375604
3522.244547	1239021.228918	41.380608
3522.225403	1238634.834863	41.385613
3522.268529	1238246.073535	41.390618
3522.137042	1237880.959169	41.395623
3522.639267	1237486.943062	41.400628
3522.204202	1237106.180080	41.405632
3522.022957	1236720.224719	41.410637
3522.579253	1236336.260397	41.415642
3522.142194	1235960.160951	41.420647
3522.081999	1235572.793970	41.425652
3522.245380	1235194.303092	41.430656
3522.271014	1234799.969413	41.435661
3522.105371	1234421.474809	41.440666
3522.064573	1234044.328890	41.445671
3522.085352	1233646.551730	41.450676
3521.921599	1233272.070674	41.455680
3521.825766	1232882.732697	41.460685
3522.124321	1232491.901755	41.465690
3521.717102	1232106.283361	41.470695
3521.919580	1231729.111060	41.475700
3521.731833	1231347.127296	41.480704
3521.354325	1230970.832991	41.485709
3521.472039	1230577.086995	41.490714
3521.481715	1230215.777246	41.495719
3521.599998	1229824.769975	41.500724
3521.413646	1229459.988277	41.505728
3521.312401	1229073.622069	41.510733
3521.664833	1228687.244952	41.515738
3521.475845	1228318.277487	41.520743
3521.559330	1227935.152093	41.525748
3521.274190	1227558.029210	41.530752
3520.950492	1227182.377418	41.535757
3521.084785	1226804.756228	41.540762
3521.225409	1226437.836970	41.545767
3521.066754	1226049.756673	41.550772
3521.081939	1225676.177206	41.555776
3520.751035	1225310.467331	41.560781
3520.999439	1224935.394912	41.565786
3520.865426	1224569.225840	41.570791
3520.864571	1224193.112810	41.575796
3521.093721	1223828.884357	41.580800
3520.810185	1223456.217693	41.585805
3520.864196	1223076.184813	41.590810
3520.854072	1222709.861282	41.595815
3521.054701	1222333.857566	41.600820
3520.772969	1221961.734716	41.605824
3520.486135	1221592.107339	41.610829
3520.822619	1221212.542424	41.615834
3520.664936	1220854.422955	41.620839
3520.725557	1220470.270689	41.625844
3520.395280	1220102.971244	41.630848
3520.255520	1219743.556034	41.635853
3520.544285	1219361.992201	41.640858
3520.408543	1219003.365061	41.645863
3520.470868	1218631.689518	41.650868
3520.547655	1218260.358326	41.655872
3520.017184	1217903.774957	41.660877
3520.020643	1217533.898412	41.665882
3519.877489	1217176.359043	41.670887
3519.883826	1216817.835066	41.675892
3520.067739	1216452.431345	41.680896
3520.231886	1216102.245793	41.685901
3520.418981	1215741.185252	41.690906
3519.617094	1215381.477741	41.695911
3519.848173	1215009.416687	41.700916
3519.628320	1214655.828219	41.705920
3519.484993	1214310.995069	41.710925
3519.785841	1213955.308050	41.715930
3519.362032	1213589.986449	41.720935
3519.492549	1213228.570328	41.725940
3519.592834	1212874.337943	41.730944
3519.323883	1212527.720896	41.735949
3519.186028	1212172.636945	41.740954
3518.822020	1211827.672407	41.745959
3519.516454	1211478.205210	41.750964
3519.047913	1211133.211010	41.755968
3519.118483	1210775.562201	41.760973
3519.276314	1210428.077231	41.765978
3518.889458	1210078.786077	41.770983
3518.680047	1209735.246293	41.775988
3518.638823	1209392.498374	41.780992
3518.860542	1209043.785329	41.785997
3519.148346	1208703.277886	41.791002
3518.755029	1208353.308140	41.796007
3519.096153	1207992.891799	41.801012
3518.725993	1207666.096907	41.806016
3518.457742	1207324.652769	41.811021
3518.526929	1206983.504974	41.816026
3518.758464	1206646.429502	41.821031
3518.509994	1206293.672172	41.826036
3518.510666	1205965.021370	41.831040
3518.772866	1205623.376484	41.836045
3519.058112	1205276.270345	41.841050
3518.376848	1204932.204831	41.846055
3518.517714	1204588.824253	41.851060
3518.391232	1204246.964246	41.856064
3518.291517	1203909.388475	41.861069
3518.637070	1203570.404903	41.866074
3518.061426	1203232.581782	41.871079
3518.100886	1202892.947701	41.876084
3518.277983	1202567.987437	41.881088
3518.292993	1202231.688682	41.886093
3518.306898	1201882.991296	41.891098
3517.844533	1201563.042219	41.896103
3517.886708	1201230.424204	41.901108
3517.963336	1200883.899279	41.906112
3517.892313	1200564.386241	41.911117
3517.816215	1200227.689923	41.916122
3517.632417	1199894.459885	41.921127
3517.701363	1199560.228562	41.926132
3517.907455	1199249.593536	41.931136
3517.652111	1198911.527176	41.936141
3518.064845	1198574.172986	41.941146
3517.342796	1198255.937227	41.946151
3517.618246	1197922.034593	41.951156
3517.577049	1197597.265115	41.956160
3517.580104	1197279.412587	41.961165
3517.700291	1196949.695596	41.966170
3517.513480	1196632.491372	41.971175
3517.387333	1196287.848897	41.976180
3517.131825	1195957.567058	41.981184
3517.075732	1195649.480177	41.986189
3517.404387	1195322.347115	41.991194
3517.069579	1195002.907581	41.996199
3517.215753	1194684.871348	42.001204
3517.157767	1194376.708685	42.006208
3517.002594	1194052.485628	42.011213
3517.074315	1193732.055219	42.016218
3517.255037	1193416.658528	42.021223
3517.083242	1193091.438603	42.026228
3516.968752	1192772.669892	42.031232
3516.799448	1192459.714512	42.036237
3516.882333	1192143.316735	42.041242
3516.636192	1191836.818170	42.046247
3516.791198	1191519.148949	42.051252
3516.987022	1191208.688250	42.056256
3516.765813	1190895.834507	42.061261
3516.675137	1190579.933282	42.066266
3516.647099	1190280.072187	42.071271
3516.940511	1189954.953897	42.076276
3516.660213	1189645.229483	42.081280
3516.528359	1189338.375814	42.086285
3516.784554	1189014.990375	42.091290
3516.565665	1188699.935295	42.096295
3516.479501	1188399.128588	42.101300
3516.715053	1188085.747418	42.106304
3516.469438	1187781.734545	42.111309
3516.503707	1187478.127837	42.116314
3516.300032	1187172.097676	42.121319
3516.296843	1186856.518629	42.126324
3516.657554	1186554.120466	42.131328
3516.087555	1186244.804286	42.136333
3516.287846	1185918.412994	42.141338
3516.343686	1185617.797381	42.146343
3515.976782	1185325.417612	42.151348
3516.205723	1185021.070309	42.156352
3515.640232	1184704.606037	42.161357
3516.069983	1184405.269612	42.166362
3515.652738	1184111.606538	42.171367
3515.867050	1183818.951915	42.176372
3516.025735	1183525.819443	42.181376
3515.681339	1183235.670445	42.186381
3515.950843	1182932.699454	42.191386
3515.674273	1182627.165500	42.196391
3515.514119	1182328.841580	42.201396
3515.501973	1182032.076246	42.206400
3515.156500	1181740.620125	42.211405
3515.475429	1181446.214139	42.216410
3515.663226	1181163.298230	42.221415
3515.553754	1180861.492509	42.226420
3515.270805	1180572.502415	42.231424
3514.942418	1180288.870639	42.236429
3515.493806	1179994.061542	42.241434
3515.090891	1179708.809596	42.246439
3515.291534	1179424.101783	42.251444
3515.691570	1179120.039125	42.256448
3515.304195	1178831.534387	42.261453
3515.348672	1178537.667958	42.266458
3515.294492	1178252.561160	42.271463
3514.911855	1177967.681210	42.276468
3515.154393	1177685.603000	42.281472
3514.972393	1177406.970922	42.286477
3515.107615	1177107.827219	42.291482
3514.748167	1176828.722302	42.296487
3514.710763	1176540.126922	42.301492
3514.882663	1176256.098314	42.306496
3514.677572	1175983.330217	42.311501
3514.837938	1175701.723346	42.316506
3514.781702	1175422.681519	42.321511
3514.500720	1175145.452488	42.326516
3514.715593	1174855.873889	42.331520
3514.463393	1174584.454044	42.336525
3514.599711	1174302.304124	42.341530
3514.499281	1174033.281442	42.346535
3514.340225	1173753.601455	42.351540
3514.359515	1173484.813550	42.356544
3514.109975	1173215.584625	42.361549
3514.569886	1172929.441375	42.366554
3514.313482	1172660.467765	42.371559
3514.184286	1172386.272839	42.376564
3514.132626	1172110.447537	42.381568
3514.150573	1171848.931229	42.386573
3514.065062	1171570.725210	42.391578
3513.964975	1171312.313802	42.396583
3514.137947	1171040.733593	42.401588
3514.133713	1170768.319469	42.406592
3514.007499	1170507.608598	42.411597
3513.872555	1170231.980645	42.416602
3513.966375	1169977.244705	42.421607
3513.693380	1169713.782382	42.426612
3514.327478	1169434.023014	42.431616
3513.438119	1169184.222289	42.436621
3513.642491	1168921.679296	42.441626
3513.864346	1168667.990726	42.446631
3513.419499	1168392.316648	42.451636
3513.682560	1168124.627836	42.456640
3513.772690	1167883.663712	42.461645
3513.665437	1167616.481755	42.466650
3513.024035	1167365.042945	42.471655
3513.435045	1167100.297781	42.476660
3513.644396	1166837.082824	42.481664
3513.293354	1166592.072588	42.486669
3513.532178	1166326.089318	42.491674
3513.244427	1166064.050215	42.496679
3513.162322	1165806.873877	42.501684
3513.128819	1165565.067856	42.506688
3513.034550	1165311.268375	42.511693
3513.084033	1165056.299717	42.516698
3513.079530	1164818.987170	42.521703
3512.954199	1164562.512253	42.526708
3512.964858	1164307.135716	42.531712
3512.614775	1164064.934701	42.536717
3512.949590	1163817.131319	42.541722
3513.187082	1163561.019840	42.546727
3512.845813	1163323.789408	42.551732
3512.921666	1163080.244653	42.556736
3513.287185	1162836.640869	42.561741
3513.180456	1162576.853528	42.566746
3512.892774	1162341.553778	42.571751
3512.598361	1162081.111386	42.576756
3513.046957	1161827.148011	42.581760
3513.035296	1161590.540692	42.586765
3512.848400	1161349.793591	42.591770
3512.867625	1161106.638899	42.596775
3512.807179	1160846.758139	42.601780
3512.618542	1160611.269849	42.606784
3512.470401	1160375.291728	42.611789
3512.705949	1160125.723295	42.616794
3512.465850	1159892.290649	42.621799
3512.260793	1159657.140307	42.626804
3512.643915	1159416.966795	42.631808
3512.377760	1159179.819905	42.636813
3512.599953	1158938.705625	42.641818
3512.113388	1158699.115196	42.646823
3512.508274	1158461.732434	42.651828
3512.534909	1158217.497041	42.656832
3512.015885	1157984.876441	42.661837
3512.215078	1157750.141403	42.666842
3512.248673	1157518.922165	42.671847
3511.987082	1157289.916520	42.676852
3512.440230	1157045.083483	42.681856
3512.006510	1156823.273650	42.686861
3511.989068	1156587.576521	42.691866
3512.001263	1156350.823455	42.696871
3512.143710	1156118.294969	42.701876
3512.266227	1155890.110959	42.706880
3512.005315	1155659.425949	42.711885
3512.135330	1155429.044850	42.716890
3511.868285	1155195.218482	42.721895
3511.433326	1154965.477767	42.726900
3512.145043	1154734.308127	42.731904
3512.037411	1154513.860964	42.736909
3511.830969	1154287.364755	42.741914
3511.980978	1154062.030280	42.746919
3511.598954	1153830.622536	42.751924
3511.865736	1153601.463721	42.756928
3511.401107	1153387.558194	42.761933
3511.957440	1153152.937541	42.766938
3511.921137	1152931.749791	42.771943
3511.705679	1152700.264887	42.776948
3512.031551	1152471.236439	42.781952
3511.761654	1152253.845023	42.786957
3511.513429	1152017.034343	42.791962
3511.738155	1151801.530797	42.796967
3511.400434	1151571.720469	42.801972
3511.652211	1151358.750577	42.806977
3511.453287	1151133.632214	42.811981
3511.571360	1150900.403620	42.816986
3511.580062	1150692.181170	42.821991
3511.474974	1150479.992053	42.826996
3511.356985	1150239.576280	42.832001
3511.475435	1150034.245424	42.837005
3511.438930	1149807.149570	42.842010
3511.221209	1149587.934772	42.847015
3510.993617	1149365.681610	42.852020
3511.033115	1149143.848682	42.857025
3510.933721	1148938.416297	42.862029
3511.040410	1148730.289636	42.867034
3511.006568	1148527.956427	42.872039
3510.850249	1148306.025772	42.877044
3511.066230	1148081.845496	42.882049
3510.640553	1147884.857459	42.887053
3510.929844	1147672.964094	42.892058
3510.956697	1147455.894251	42.897063
3510.774793	1147252.115251	42.902068
3511.135587	1147044.448749	42.907073
3511.162418	1146845.736527	42.912077
3511.159856	1146628.732269	42.917082
3510.848765	1146412.907114	42.922087
3510.529468	1146197.737886	42.927092
3510.831432	1145988.238871	42.932097
3510.558083	1145787.545969	42.937101
3510.623641	1145578.259185	42.942106
3510.577275	1145374.290581	42.947111
3510.465682	1145177.528883	42.952116
3510.779182	1144978.035629	42.957121
3510.776988	1144787.308162	42.962125
3510.642840	1144568.439764	42.967130
3510.557009	1144364.059453	42.972135
3510.321087	1144154.765927	42.977140
3510.218120	1143956.061151	42.982145
3510.145083	1143767.963289	42.987149
3509.832000	1143563.020532	42.992154
3509.915481	1143376.968995	42.997159
3509.984405	1143190.723659	43.002164
3509.979931	1142991.018131	43.007169
3510.126813	1142803.798040	43.012173
3509.951555	1142611.882581	43.017178
3510.064166	1142418.015960	43.022183
3510.043845	1142228.906270	43.027188
3510.111888	1142034.179339	43.032193
3509.954125	1141850.769543	43.037197
3509.987949	1141650.627704	43.042202
3510.121083	1141458.714472	43.047207
3509.868357	1141275.869527	43.052212
3510.082931	1141073.778909	43.057217
3509.995111	1140880.268414	43.062221
3509.826375	1140688.946190	43.067226
3509.934358	1140503.074158	43.072231
3509.336319	1140321.201835	43.077236
3509.672276	1140134.140784	43.082241
3509.904983	1139954.965474	43.087245
3509.810820	1139756.670776	43.092250
3509.609337	1139581.919161	43.097255
3509.611423	1139405.325278	43.102260
3510.139008	1139211.937142	43.107265
3509.683486	1139017.659958	43.112269
3509.725395	1138830.791120	43.117274
3509.526117	1138650.409090	43.122279
3509.368440	1138463.275441	43.127284
3509.588813	1138277.591540	43.132289
3509.461275	1138098.128031	43.137293
3509.528536	1137905.242624	43.142298
3509.473444	1137739.043847	43.147303
3509.117717	1137559.789538	43.152308
3509.399459	1137379.285025	43.157313
3509.276561	1137200.644736	43.162317
3509.461307	1137035.238797	43.167322
3509.258342	1136851.283516	43.172327
3509.481441	1136665.068009	43.177332
3509.481345	1136475.749513	43.182337
3509.113566	1136313.450331	43.187341
3509.079988	1136125.454131	43.192346
3509.519344	1135949.907491	43.197351
3508.954681	1135764.929594	43.202356
3509.279960	1135596.986752	43.207361
3509.244360	1135418.272060	43.212365
3508.925188	1135230.101246	43.217370
3509.183484	1135072.029509	43.222375
3509.103056	1134891.215093	43.227380
3509.069389	1134723.968573	43.232385
3508.692981	1134555.443509	43.237389
3508.547402	1134374.527244	43.242394
3508.859346	1134209.772162	43.247399
3508.666136	1134055.543984	43.252404
3509.111519	1133885.912436	43.257409
3508.697989	1133716.701916	43.262413
3508.950671	1133546.521300	43.267418
3508.767006	1133368.996992	43.272423
3508.522633	1133208.197532	43.277428
3508.765564	1133041.992545	43.282433
3508.455932	1132876.348415	43.287437
3508.603827	1132702.642655	43.292442
3508.554675	1132551.007440	43.297447
3508.419425	1132375.057221	43.302452
3508.395626	1132221.983156	43.307457
3508.680175	1132066.668334	43.312461
3508.730740	1131913.478117	43.317466
3508.590802	1131735.797018	43.322471
3508.356608	1131575.611693	43.327476
3508.476291	1131411.276696	43.332481
3508.371626	1131251.155301	43.337485
3508.292735	1131093.210808	43.342490
3508.662978	1130918.649815	43.347495
3508.190661	1130762.281012	43.352500
3508.242291	1130607.152032	43.357505
3508.495442	1130450.654590	43.362509
3508.662143	1130297.208588	43.367514
3508.512551	1130133.829044	43.372519
3508.370759	1129971.393819	43.377524
3508.413017	1129819.665662	43.382529
3508.406184	1129651.684689	43.387533
3508.066346	1129489.932858	43.392538
3507.848915	1129338.709113	43.397543
3508.002767	1129188.370685	43.402548
3508.484569	1129034.551165	43.407553
3508.019308	1128868.807800	43.412557
3508.131126	1128714.754732	43.417562
3508.247014	1128583.327276	43.422567
3507.792156	1128420.801202	43.427572
3508.115708	1128262.991694	43.432577
3508.011116	1128121.414229	43.437581
3508.022587	1127961.364900	43.442586
3508.068145	1127807.581804	43.447591
3508.252658	1127657.575524	43.452596
3507.929484	1127499.374396	43.457601
3507.924685	1127349.580837	43.462605
3507.665734	1127195.830234	43.467610
3507.942265	1127059.202690	43.472615
3507.676238	1126909.630015	43.477620
3507.729954	1126748.395893	43.482625
3507.915454	1126621.759689	43.487629
3507.737289	1126470.923645	43.492634
3507.898820	1126322.690952	43.497639
3507.769478	1126171.172495	43.502644
3507.910214	1126020.746844	43.507649
3507.755048	1125872.363525	43.512653
3507.720442	1125728.142289	43.517658
3507.427432	1125585.101395	43.522663
3507.424503	1125434.112016	43.527668
3507.576408	1125300.789955	43.532673
3507.749321	1125154.616125	43.537677
3507.594735	1125008.301926	43.542682
3507.853573	1124857.253110	43.547687
3507.273988	1124724.703198	43.552692
3507.749521	1124578.083114	43.557697
3507.510077	1124431.100950	43.562701
3507.544039	1124295.869986	43.567706
3507.469005	1124152.374113	43.572711
3506.950460	1124012.087984	43.577716
3507.403159	1123871.923722	43.582721
3507.006661	1123743.030924	43.587725
3507.075996	1123615.390750	43.592730
3507.349542	1123477.720212	43.597735
3507.071155	1123340.993649	43.602740
3507.327136	1123196.560940	43.607745
3506.930553	1123057.657375	43.612749
3506.876868	1122924.024246	43.617754
3507.005147	1122806.540124	43.622759
3507.039553	1122683.071776	43.627764
3507.150796	1122540.358621	43.632769
3506.996490	1122408.347470	43.637773
3506.898758	1122274.705348	43.642778
3507.072673	1122142.062365	43.647783
3506.871731	1122019.855070	43.652788
3507.000914	1121884.642556	43.657793
3507.286645	1121741.593710	43.662797
3507.057358	1121603.767275	43.667802
3507.226739	1121477.011637	43.672807
3506.932986	1121348.520165	43.677812
3506.946073	1121208.929740	43.682817
3507.093466	1121074.265037	43.687821
3507.062086	1120953.624182	43.692826
3507.039734	1120813.743606	43.697831
3506.697245	1120690.386506	43.702836
3507.000574	1120555.683061	43.707841
3506.919380	1120437.229047	43.712845
3506.843576	1120296.867589	43.717850
3507.068620	1120166.262320	43.722855
3506.395953	1120053.706673	43.727860
3506.459105	1119921.693507	43.732865
3506.885799	1119801.617906	43.737869
3506.853990	1119674.757434	43.742874
3507.113030	1119550.227252	43.747879
3506.797768	1119414.739722	43.752884
3506.792619	1119273.006249	43.757889
3506.630507	1119158.061583	43.762893
3506.522413	1119033.579841	43.767898
3506.842821	1118907.024184	43.772903
3506.476638	1118786.199048	43.777908
3506.790947	1118666.592802	43.782913
3506.510338	1118539.460592	43.787917
3506.300067	1118415.362357	43.792922
3506.542290	1118292.425237	43.797927
3506.356282	1118175.081627	43.802932
3505.996681	1118054.429422	43.807937
3506.315916	1117946.334490	43.812941
3506.579647	1117826.146142	43.817946
3506.430915	1117706.308869	43.822951
3506.249679	1117592.858219	43.827956
3506.304591	1117459.261133	43.832961
3506.326019	1117341.388656	43.837965
3506.230684	1117222.770499	43.842970
3506.353181	1117117.645218	43.847975
3506.099395	1117008.768118	43.852980
3506.584333	1116882.232804	43.857985
3506.503782	1116775.895416	43.862989
3506.286390	1116646.230086	43.867994
3506.417505	1116518.886768	43.872999
3506.114747	1116418.773507	43.878004
3506.343319	1116291.980569	43.883009
3506.271745	1116193.635838	43.888013
3506.210380	1116066.408774	43.893018
3506.350393	1115960.590735	43.898023
3505.961941	1115835.890174	43.903028
3506.266450	1115720.985469	43.908033
3506.454811	1115608.003793	43.913037
3506.295854	1115499.080383	43.918042
3506.395512	1115374.574656	43.923047
3506.103877	1115267.098215	43.928052
3506.118913	1115161.856936	43.933057
3506.274424	1115044.007155	43.938061
3505.989233	1114915.645695	43.943066
3506.060963	1114811.532167	43.948071
3505.893560	1114702.975296	43.953076
3506.044041	1114588.167018	43.958081
3506.250961	1114486.980349	43.963085
3506.164309	1114370.585722	43.968090
3506.327505	1114248.617569	43.973095
3506.148201	1114135.188701	43.978100
3506.005596	1114023.086238	43.983105
3506.361709	1113908.515588	43.988109
3506.259580	1113794.304014	43.993114
3506.298953	1113681.306284	43.998119
3506.241023	1113575.378420	44.003124
3506.375678	1113449.868700	44.008129
3506.107502	1113341.205498	44.013133
3506.112216	1113239.170372	44.018138
3506.139289	1113109.474556	44.023143
3505.833915	1113010.060930	44.028148
3505.579568	1112899.097748	44.033153
3505.851733	1112788.045558	44.038157
3506.130130	1112686.527061	44.043162
3506.060188	1112572.951772	44.048167
3505.847079	1112465.596972	44.053172
3505.780281	1112352.493370	44.058177
3505.808278	1112252.152411	44.063181
3505.616985	1112144.787599	44.068186
3506.086987	1112028.441233	44.073191
3505.789601	1111932.630831	44.078196
3505.989963	1111821.093553	44.083201
3505.673141	1111718.414771	44.088205
3505.499627	1111608.651625	44.093210
3505.315805	1111508.617821	44.098215
3505.132213	1111423.940330	44.103220
3505.428397	1111324.587184	44.108225
3505.577291	1111230.503239	44.113229
3505.328001	1111123.986125	44.118234
3505.541549	1111023.877847	44.123239
3505.513542	1110939.357889	44.128244
3505.403495	1110827.660303	44.133249
3505.554183	1110722.023372	44.138253
3505.344100	1110639.532187	44.143258
3505.483993	1110533.893337	44.148263
3505.477424	1110438.485410	44.153268
3505.520769	1110334.194275	44.158273
3505.432148	1110247.288115	44.163277
3504.922157	1110140.221941	44.168282
3505.372973	1110041.487516	44.173287
3505.172049	1109962.133180	44.178292
3505.207841	1109855.543955	44.183297
3505.142333	1109757.175607	44.188301
3505.109561	1109670.060068	44.193306
3505.276138	1109572.413505	44.198311
3505.164310	1109475.192728	44.203316
3505.478225	1109389.542380	44.208321
3505.754421	1109296.262465	44.213325
3505.314126	1109185.348565	44.218330
3505.359961	1109096.588438	44.223335
3505.369794	1109005.446890	44.228340
3505.349054	1108898.466258	44.233345
3505.139595	1108805.544127	44.238349
3504.734328	1108717.138345	44.243354
3505.106136	1108623.926464	44.248359
3505.179511	1108534.007208	44.253364
3505.691775	1108439.337342	44.258369
3505.380064	1108354.441669	44.263373
3504.997209	1108253.998243	44.268378
3505.278952	1108152.966233	44.273383
3505.079507	1108068.429355	44.278388
3504.971650	1107961.921699	44.283393
3504.951551	1107872.293139	44.288397
3505.166850	1107797.992894	44.293402
3505.132502	1107694.617914	44.298407
3505.099966	1107621.215174	44.303412
3505.140160	1107522.024840	44.308417
3504.771179	1107438.842451	44.313421
3504.704313	1107349.403807	44.318426
3504.904456	1107269.275403	44.323431
3504.513072	1107186.665598	44.328436
3504.644895	1107103.395541	44.333441
3504.891760	1107017.909423	44.338445
3504.603679	1106929.932300	44.343450
3504.997625	1106856.830782	44.348455
3504.714487	1106768.563786	44.353460
3504.720318	1106669.745302	44.358465
3504.724442	1106594.126544	44.363469
3504.520415	1106514.244422	44.368474
3504.872136	1106418.419708	44.373479
3504.926752	1106339.256244	44.378484
3504.824677	1106255.725150	44.383489
3505.108723	1106168.214252	44.388493
3504.989522	1106076.280440	44.393498
3505.068970	1105988.609345	44.398503
3504.846250	1105911.204064	44.403508
3505.071013	1105818.636262	44.408513
3505.304172	1105728.070852	44.413517
3504.845147	1105647.835893	44.418522
3505.213725	1105565.076025	44.423527
3505.104365	1105473.607784	44.428532
3504.559134	1105392.141733	44.433537
3504.940279	1105302.117788	44.438541
3504.722786	1105206.651771	44.443546
3504.847612	1105119.914091	44.448551
3504.372930	1105039.195113	44.453556
3504.523012	1104957.703478	44.458561
3504.626583	1104877.650901	44.463565
3504.246792	1104806.272642	44.468570
3504.925793	1104721.347477	44.473575
3504.857500	1104632.436993	44.478580
3505.002898	1104550.844465	44.483585
3505.142793	1104465.813036	44.488589
3504.813473	1104383.723066	44.493594
3504.612370	1104299.413792	44.498599
3504.671887	1104228.528636	44.503604
3504.867812	1104134.503850	44.508609
3505.094921	1104047.541022	44.513613
3504.520142	1103962.428306	44.518618
3504.720749	1103882.249439	44.523623
3504.912398	1103796.339189	44.528628
3505.111107	1103717.400046	44.533633
3504.956521	1103633.932461	44.538637
3504.705911	1103547.422367	44.543642
3504.984903	1103467.893156	44.548647
3504.877674	1103375.815740	44.553652
3504.988799	1103297.075939	44.558657
3505.117379	1103210.211373	44.563661
3504.897048	1103118.721422	44.568666
3504.848116	1103021.087032	44.573671
3504.797914	1102939.120161	44.578676
3504.669568	1102852.865410	44.583681
3504.911342	1102772.472176	44.588685
3504.742167	1102693.769731	44.593690
3504.558818	1102598.920707	44.598695
3504.421720	1102533.778589	44.603700
3504.524215	1102465.825235	44.608705
3504.754708	1102376.350566	44.613709
3504.238768	1102294.355044	44.618714
3504.290287	1102220.864839	44.623719
3504.212041	1102154.561778	44.628724
3504.331751	1102078.191691	44.633729
3504.660716	1101984.776423	44.638733
3504.233609	1101921.299186	44.643738
3504.577188	1101847.946925	44.648743
3504.358461	1101770.385910	44.653748
3504.347129	1101693.649708	44.658753
3504.115716	1101616.661962	44.663757
3504.388669	1101546.279793	44.668762
3504.522518	1101471.714581	44.673767
3504.568605	1101403.183721	44.678772
3504.407668	1101316.909771	44.683777
3504.726034	1101240.208395	44.688781
3504.651554	1101167.871478	44.693786
3504.619547	1101076.984886	44.698791
3504.318571	1101006.594629	44.703796
3504.449314	1100929.537432	44.708801
3504.415667	1100851.932729	44.713805
3504.112538	1100785.458718	44.718810
3504.215016	1100713.277726	44.723815
3504.318906	1100650.080398	44.728820
3504.324438	1100572.656394	44.733825
3504.521293	1100495.868875	44.738829
3504.188101	1100441.248260	44.743834
3504.439783	1100347.148277	44.748839
3504.272077	1100273.094120	44.753844
3503.969171	1100198.105297	44.758849
3504.244690	1100128.086590	44.763853
3504.216224	1100065.860151	44.768858
3504.491080	1099986.375914	44.773863
3503.954992	1099929.680437	44.778868
3504.241787	1099852.390976	44.783873
3504.368956	1099771.589534	44.788877
3504.185923	1099697.530005	44.793882
3504.556676	1099623.569458	44.798887
3504.107722	1099570.297514	44.803892
3503.972946	1099483.320723	44.808897
3504.429870	1099410.968347	44.813901
3503.883507	1099344.325428	44.818906
3504.260643	1099268.542446	44.823911
3504.289473	1099199.986462	44.828916
3504.228991	1099137.850213	44.833921
3504.451966	1099070.885992	44.838925
3503.701418	1098997.579608	44.843930
3504.161201	1098915.658845	44.848935
3504.308357	1098846.122741	44.853940
3504.091155	1098782.287133	44.858945
3504.195712	1098702.047120	44.863949
3503.846549	1098658.215911	44.868954
3504.356695	1098571.309458	44.873959
3504.051262	1098507.676376	44.878964
3503.961453	1098438.939032	44.883969
3504.114181	1098376.663291	44.888973
3503.674537	1098307.981895	44.893978
3504.432159	1098229.539813	44.898983
3504.261776	1098166.741110	44.903988
3503.965038	1098091.243865	44.908993
3503.978432	1098019.902215	44.913997
3504.056053	1097961.172370	44.919002
3504.584202	1097885.918929	44.924007
3504.231161	1097821.138009	44.929012
3503.955001	1097754.048415	44.934017
3504.513723	1097687.107396	44.939021
3504.205248	1097610.744646	44.944026
3504.034792	1097534.645002	44.949031
3504.357796	1097475.773834	44.954036
3504.163229	1097392.694458	44.959041
3504.240590	1097318.655065	44.964045
3504.104583	1097263.969815	44.969050
3504.034152	1097175.032393	44.974055
3503.894005	1097116.807468	44.979060
3503.964429	1097054.912645	44.984065
3503.985431	1096980.877909	44.989069
3503.843492	1096912.607980	44.994074
3503.941278	1096846.880281	44.999079
3503.896087	1096782.514459	45.004084
3504.110584	1096722.505144	45.009089
3503.882859	1096662.185378	45.014093
3503.946053	1096588.999217	45.019098
3504.015727	1096515.810999	45.024103
3504.126854	1096453.424306	45.029108
3503.972680	1096386.680277	45.034113
3503.852358	1096319.355887	45.039117
3503.959616	1096257.924179	45.044122
3504.159240	1096194.276328	45.049127
3503.877870	1096125.923767	45.054132
3503.745673	1096068.738545	45.059137
3503.721330	1096003.212040	45.064141
3503.463669	1095935.905495	45.069146
3503.602892	1095878.386558	45.074151
3503.829021	1095839.029776	45.079156
3503.625460	1095774.486703	45.084161
3503.849679	1095710.542103	45.089165
3503.641693	1095651.068844	45.094170
3504.003584	1095583.655880	45.099175
3504.010506	1095521.466953	45.104180
3503.599650	1095456.284503	45.109185
3503.707397	1095391.494239	45.114189
3503.714369	1095332.173424	45.119194
3503.834565	1095260.299391	45.124199
3503.544757	1095215.856388	45.129204
3503.594398	1095156.335260	45.134209
3503.678023	1095077.384441	45.139213
3503.821063	1095036.983012	45.144218
3503.770859	1094976.615207	45.149223
3503.675643	1094914.436125	45.154228
3503.579168	1094872.159213	45.159233
3503.861841	1094808.959827	45.164237
3503.463423	1094745.871875	45.169242
3503.597996	1094672.169594	45.174247
3503.397211	1094630.577798	45.179252
3503.776618	1094578.172752	45.184257
3503.822068	1094500.463791	45.189261
3503.421328	1094444.166854	45.194266
3503.413873	1094390.675388	45.199271
3503.475511	1094327.698179	45.204276
3503.379831	1094276.038322	45.209281
3503.595590	1094223.274011	45.214285
3502.932516	1094162.710972	45.219290
3503.329781	1094112.690941	45.224295
3503.182061	1094064.961306	45.229300
3503.472810	1094006.536229	45.234305
3503.788601	1093956.623879	45.239309
3503.484706	1093906.047505	45.244314
3503.558435	1093841.435703	45.249319
3503.367460	1093796.103420	45.254324
3503.010400	1093740.366192	45.259329
3503.226360	1093678.791609	45.264333
3503.143808	1093642.245204	45.269338
3503.480531	1093587.444923	45.274343
3503.305015	1093537.992467	45.279348
3503.169738	1093487.767250	45.284353
3503.619134	1093422.227186	45.289357
3503.611623	1093372.745552	45.294362
3503.460838	1093308.068653	45.299367
3503.365499	1093264.726151	45.304372
3503.321349	1093202.710427	45.309377
3503.731400	1093146.075019	45.314381
3503.496688	1093102.562741	45.319386
3503.413979	1093034.521266	45.324391
3503.379882	1092976.904338	45.329396
3503.476761	1092937.739208	45.334401
3503.809189	1092877.667863	45.339405
3503.673774	1092822.746171	45.344410
3503.543251	1092764.664258	45.349415
3503.605366	1092703.582550	45.354420
3503.480081	1092657.847021	45.359425
3503.430507	1092597.835489	45.364429
3503.222727	1092546.560499	45.369434
3503.321505	1092482.598456	45.374439
3503.562568	1092437.949471	45.379444
3503.499325	1092396.030664	45.384449
3503.557254	1092328.531538	45.389453
3503.381546	1092280.024933	45.394458
3503.553873	1092208.006080	45.399463
3503.426543	1092161.117900	45.404468
3503.194101	1092110.895918	45.409473
3503.586536	1092056.741137	45.414477
3503.345014	1092003.264645	45.419482
3503.382732	1091938.253135	45.424487
3503.327772	1091899.488462	45.429492
3503.113957	1091861.611325	45.434497
3503.373518	1091802.018763	45.439501
3503.402828	1091752.037565	45.444506
3503.592346	1091695.519077	45.449511
3503.221157	1091648.762368	45.454516
3502.813848	1091595.883613	45.459521
3502.946637	1091535.351564	45.464525
3502.762651	1091505.605318	45.469530
3503.016921	1091447.158673	45.474535
3503.203687	1091422.616954	45.479540
3503.060372	1091364.617886	45.484545
3503.333388	1091316.698988	45.489549
3503.216656	1091265.205377	45.494554
3503.348826	1091204.956992	45.499559
3503.113915	1091159.131117	45.504564
3503.092862	1091120.355288	45.509569
3503.201389	1091066.811901	45.514573
3503.169234	1091016.068018	45.519578
3503.359199	1090974.575284	45.524583
3503.231155	1090920.590643	45.529588
3503.139785	1090874.834479	45.534593
3503.264352	1090819.562395	45.539597
3503.055562	1090786.177505	45.544602
3503.021118	1090726.142758	45.549607
3502.927236	1090681.247205	45.554612
3502.729835	1090637.804737	45.559617
3502.995613	1090597.254238	45.564621
3502.477618	1090554.725755	45.569626
3502.805292	1090513.302577	45.574631
3502.829500	1090470.396846	45.579636
3502.589021	1090437.589608	45.584641
3502.900885	1090385.442470	45.589645
3502.610446	1090347.854663	45.594650
3503.181012	1090316.924200	45.599655
3503.221095	1090276.791544	45.604660
3503.017798	1090227.888045	45.609665
3503.022353	1090175.502200	45.614669
3502.705189	1090146.345038	45.619674
3502.765358	1090090.501519	45.624679
3502.994523	1090047.846002	45.629684
3502.553701	1090010.089078	45.634689
3502.317519	1089969.137701	45.639693
3502.508655	1089939.608395	45.644698
3503.150520	1089900.427348	45.649703
3502.857277	1089858.909894	45.654708
3502.835851	1089812.845927	45.659713
3503.179162	1089766.051067	45.664717
3502.425922	1089731.216930	45.669722
3503.106223	1089674.692341	45.674727
3502.826032	1089634.990797	45.679732
3502.597379	1089613.382666	45.684737
3503.260700	1089561.648629	45.689741
3502.922396	1089517.741495	45.694746
3502.746530	1089482.235982	45.699751
3502.934988	1089427.322321	45.704756
3502.881430	1089390.359335	45.709761
3503.065187	1089347.801582	45.714765
3503.088443	1089306.994043	45.719770
3503.169853	1089250.372110	45.724775
3503.074664	1089224.142763	45.729780
3502.864972	1089166.610044	45.734785
3503.132449	1089114.649589	45.739789
3502.707250	1089074.488884	45.744794
3502.908186	1089041.887864	45.749799
3502.845353	1088994.770097	45.754804
3502.814089	1088948.891996	45.759809
3503.032156	1088906.037761	45.764813
3502.992005	1088852.688598	45.769818
3502.943874	1088746.653818	45.774823
3503.010691	1088580.629532	45.779828
3502.528030	1088351.749840	45.784833
3502.901328	1088071.080415	45.789837
3502.750011	1087730.121754	45.794842
3502.757210	1087320.413729	45.799847
3502.521506	1086847.564905	45.804852
3502.543628	1086323.647600	45.809857
3502.329414	1085717.482315	45.814861
3502.333136	1085063.763614	45.819866
3502.178532	1084331.953353	45.824871
3502.472121	1083531.508754	45.829876
3501.949183	1082666.539863	45.834881
3501.673153	1081720.918465	45.839885
3501.596534	1080719.170004	45.844890
3501.520671	1079644.312491	45.849895
3501.146135	1078490.401716	45.854900
3500.888753	1077253.863298	45.859905
3501.255461	1075963.171561	45.864909
3500.804242	1074585.583189	45.869914
3500.704599	1073118.246182	45.874919
3500.362644	1071565.318648	45.879924
3500.280466	1069951.157249	45.884929
3500.165367	1068234.121729	45.889933
3499.997618	1066456.537358	45.894938
3499.246020	1064602.846044	45.899943
3499.252182	1062649.457289	45.904948
3498.849372	1060620.626269	45.909953
3498.384667	1058500.126936	45.914957
3497.690498	1056305.034779	45.919962
3497.118560	1054044.169403	45.924967
3497.136521	1051702.714815	45.929972
3496.375970	1049280.216568	45.934977
3496.465905	1046748.307571	45.939981
3495.781758	1044169.881550	45.944986
3495.326319	1041483.742077	45.949991
3495.048482	1038716.617745	45.954996
3494.559183	1035887.894701	45.960001
3494.006051	1032964.265176	45.965005
3493.606024	1029967.331828	45.970010
3492.816328	1026881.859570	45.975015
3492.625141	1023727.219011	45.980020
3491.685635	1020484.218458	45.985025
3491.591670	1017141.479626	45.990029
3490.934074	1013743.242715	45.995034
3490.268855	1010253.272412	46.000039
3489.602957	1006683.943673	46.005044
3488.657620	1003022.995862	46.010049
3488.427826	999283.916274	46.015053
3487.563980	995475.448472	46.020058
3486.961219	991579.861450	46.025063
3486.317511	987607.080123	46.030068
3485.506390	983543.693936	46.035073
3484.969792	979392.765126	46.040077
3484.031000	975187.168874	46.045082
3483.317942	970890.782832	46.050087
3482.753365	966505.872063	46.055092
3481.971043	962034.067091	46.060097
3481.183967	957485.534830	46.065101
3480.247633	952908.549004	46.070106
3479.634533	948318.969490	46.075111
3478.668790	943643.231282	46.080116
3477.440473	938894.650678	46.085121
3477.029532	934065.789767	46.090125
3476.019153	929159.877275	46.095130
3474.939614	924151.941049	46.100135
3474.263195	919089.127761	46.105140
3472.684524	913937.727447	46.110145
3472.204468	908697.309417	46.115149
3470.849387	903394.454243	46.120154
3469.929824	898001.670598	46.125159
3468.761237	892526.417965	46.130164
3467.599785	886970.898999	46.135169
3466.245265	881347.868515	46.140173
3464.972499	875648.227284	46.145178
3463.491786	869860.508400	46.150183
3462.802143	863997.774976	46.155188
3461.286433	858069.001934	46.160193
3460.102392	852050.703581	46.165197
3459.114152	845949.347827	46.170202
3457.886625	839780.651540	46.175207
3456.533964	833527.243509	46.180212
3455.227038	827201.496566	46.185217
3454.164404	820774.778062	46.190221
3452.964934	814278.488871	46.195226
3451.609583	807715.366683	46.200231
3450.222321	801042.355072	46.205236
3448.658921	794302.532691	46.210241
3447.301458	787485.223835	46.215245
3445.998776	780597.914028	46.220250
3444.594034	773617.186246	46.225255
3443.104466	766568.570362	46.230260
3441.399721	759446.381761	46.235265
3439.823579	752226.018607	46.240269
3438.285920	744948.626732	46.245274
3436.582382	737593.910720	46.250279
3435.290694	730150.242420	46.255284
3433.523579	722633.121031	46.260289
3431.985042	715043.402872	46.265293
3430.510583	707371.614662	46.270298
3428.643093	699618.245593	46.275303
3427.012686	691804.213360	46.280308
3425.152973	683914.039622	46.285313
3423.529874	675940.716555	46.290317
3421.801844	667890.621608	46.295322
3419.656502	659782.187994	46.300327
3418.362778	651597.625281	46.305332
3416.076493	643335.857142	46.310337
3414.163882	634999.784635	46.315341
3412.223486	626599.779343	46.320346
3410.090555	618126.560422	46.325351
3408.086249	609599.290522	46.330356
3406.178464	601005.874653	46.335361
3404.683187	592325.889386	46.340365
3402.234354	583598.868977	46.345370
3400.166040	574792.975112	46.350375
3398.538488	565889.990216	46.355380
3396.062567	556953.803482	46.360385
3394.014421	547953.272172	46.365389
3391.754065	538871.013582	46.370394
3389.571992	529718.633044	46.375399
3387.468700	520528.985270	46.380404
3385.057769	511266.183497	46.385409
3382.920621	501914.786828	46.390413
3380.505790	492536.932348	46.395418
3377.929970	483097.484725	46.400423
3375.562625	473574.417751	46.405428
3372.854975	464012.207620	46.410433
3370.726806	454391.196811	46.415437
3367.959565	444717.867865	46.420442
3365.024240	434988.293342	46.425447
3362.722932	425195.191205	46.430452
3359.991802	415352.252736	46.435457
3357.338587	405447.357371	46.440461
3354.613973	395523.421839	46.445466
3351.824053	385537.965073	46.450471
3348.965550	375493.363401	46.455476
3345.743634	365415.654565	46.460481
3343.172640	355296.197378	46.465485
3340.200063	345137.247946	46.470490
3336.647467	334931.763287	46.475495
3333.593282	324682.726889	46.480500
3330.462096	314419.040623	46.485505
3327.590417	304123.822582	46.490509
3324.219989	293768.983829	46.495514
3320.728437	283398.620948	46.500519
3317.563004	272984.151127	46.505524
3314.010280	262551.939712	46.510529
3310.227510	252094.927928	46.515533
3306.770844	241614.348307	46.520538
3302.910893	231086.310655	46.525543
3299.707231	220511.341935	46.530548
3295.638042	209966.897832	46.535553
3291.410464	199416.366087	46.540557
3287.435575	188875.749986	46.545562
3283.323518	178332.418038	46.550567
3278.870389	167766.454888	46.555572
3274.343950	157203.265007	46.560577
3269.800092	146658.359440	46.565581
3264.973442	136124.354389	46.570586
3259.991648	125607.429743	46.575591
3255.003215	115101.165198	46.580596
3249.282016	104656.394447	46.585601
3243.990160	94219.025315	46.590605
3238.292455	83827.027353	46.595610
3231.678093	73505.040463	46.600615
3225.336857	63230.358320	46.605620
3217.246737	53048.115061	46.610625
3208.271533	42994.616665	46.615629
3194.871194	33152.962927	46.620634
3166.702161	23877.551981	46.625639
3125.144177	15308.065127	46.630644
3068.133856	7716.050976	46.635649
2988.094177	1624.440434	46.640653
2777.641697	422.677636	46.645658
2615.942320	397.393868	46.650663
2570.405887	380.166751	46.655668
2612.525549	381.056602	46.660673
2695.055855	381.501015	46.665677
2776.788914	375.846154	46.670682
2833.443929	373.906076	46.675687
2860.867209	351.340887	46.680692
2863.591844	361.038716	46.685697
2853.668179	359.424786	46.690701
2840.102144	362.442625	46.695706
2828.445612	363.578598	46.700711
2821.289538	351.288205	46.705716
2817.475271	344.337415	46.710721
2815.543933	348.585722	46.715725
2815.078482	338.498395	46.720730
2813.481302	355.258549	46.725735
2811.754733	349.138708	46.730740
2809.379709	338.368359	46.735745
2806.653741	328.435574	46.740749
2803.631670	331.608564	46.745754
2800.459198	339.905220	46.750759
2797.448436	329.987522	46.755764
2793.965111	328.704878	46.760769
2791.257671	330.820080	46.765773
2788.487428	318.528089	46.770778
2785.220679	327.134090	46.775783
2782.165701	313.605206	46.780788
2778.584750	323.113739	46.785793
2775.580917	319.617382	46.790797
2772.784553	316.391284	46.795802
2769.176864	316.985117	46.800807
2765.785949	315.949487	46.805812
2762.212538	306.538060	46.810817
2758.986816	311.298998	46.815821
2755.909887	315.749891	46.820826
2752.754430	310.495591	46.825831
2749.553292	303.577653	46.830836
2745.963714	310.350438	46.835841
2742.764369	311.117293	46.840845
2739.666015	311.727897	46.845850
2736.198654	317.391845	46.850855
2732.472048	298.207745	46.855860
2729.255696	302.028611	46.860865
2726.056781	296.071352	46.865869
2722.717571	296.257683	46.870874
2719.307242	302.826002	46.875879
2715.715765	300.018411	46.880884
2712.462920	300.951754	46.885889
2709.221725	294.869272	46.890893
2705.995461	298.713288	46.895898
2702.047156	298.164613	46.900903
2699.064614	289.221027	46.905908
2695.758192	295.304383	46.910913
2691.721594	292.827791	46.915917
2689.056794	287.702676	46.920922
2685.411560	303.738789	46.925927
2682.322458	285.889153	46.930932
2678.379959	289.616953	46.935937
2674.806586	295.921816	46.940941
2671.313022	285.442141	46.945946
2667.608480	284.567778	46.950951
2665.090259	283.940695	46.955956
2661.804309	286.346462	46.960961
2658.089738	280.822327	46.965965
2653.966089	284.372232	46.970970
2650.871987	283.794228	46.975975
2647.868690	277.806931	46.980980
2644.362438	286.971486	46.985985
2640.651051	279.570164	46.990989
2637.241223	283.203939	46.995994
2633.733770	281.825413	47.000999
2630.494311	276.591346	47.006004
2626.720514	278.806748	47.011009
2623.208577	280.132786	47.016013
2619.754705	268.218829	47.021018
2616.393503	279.705460	47.026023
2613.743921	277.937173	47.031028
2609.197198	282.093655	47.036033
2606.150380	271.487582	47.041037
2602.725769	273.627760	47.046042
2599.240481	278.886358	47.051047
2595.861860	280.644746	47.056052
2592.666727	276.388785	47.061057
2589.251908	276.549361	47.066061
2585.286975	274.664603	47.071066
2581.839143	266.805500	47.076071
2578.787807	265.816669	47.081076
2575.207530	278.257741	47.086081
2571.595164	271.289323	47.091085
2568.185971	270.309286	47.096090
2564.742795	274.519619	47.101095
2561.088853	259.148474	47.106100
2557.028228	275.969742	47.111105
2553.806469	276.382832	47.116109
2550.656798	259.458738	47.121114
2547.351013	271.701831	47.126119
2543.988092	273.364716	47.131124
2540.240000	271.009541	47.136129
2536.804147	278.429400	47.141133
2533.096952	270.522026	47.146138
2529.428098	262.609915	47.151143
2526.564597	265.512371	47.156148
2523.043442	259.512168	47.161153
2519.481339	265.621065	47.166157
2516.031184	266.573013	47.171162
2512.189673	261.293850	47.176167
2509.107772	263.222562	47.181172
2505.499184	265.322182	47.186177
2501.876523	262.576477	47.191181
2498.924547	261.596946	47.196186
2495.052119	261.689081	47.201191
2491.801455	260.055574	47.206196
2488.027928	260.583257	47.211201
2484.256232	265.584964	47.216205
2480.742170	262.508617	47.221210
2477.623189	261.074986	47.226215
2474.367497	249.272489	47.231220
2470.763118	244.126212	47.236225
2466.987399	262.226275	47.241229
2463.968554	243.978889	47.246234
2460.106067	249.947323	47.251239
2456.952130	253.841058	47.256244
2453.553293	249.440092	47.261249
2449.786856	257.396924	47.266253
2446.582811	242.879652	47.271258
2442.321451	249.235988	47.276263
2439.534259	245.492842	47.281268
2435.683483	246.950410	47.286273
2432.135772	252.778059	47.291277
2428.812315	246.521949	47.296282
2424.738303	257.254137	47.301287
2421.804820	257.220969	47.306292
2418.609309	254.643422	47.311297
2414.962953	256.921862	47.316301
2411.700039	246.833288	47.321306
2407.835168	247.812140	47.326311
2404.171609	256.371790	47.331316
2400.865921	248.005240	47.336321
2397.249416	249.491872	47.341325
2394.158284	249.756021	47.346330
2390.199814	248.776477	47.351335
2386.827821	235.657987	47.356340
2383.542992	254.973373	47.361345
2379.957649	248.152745	47.366349
2376.951113	244.557084	47.371354
2373.068215	255.612154	47.376359
2369.599278	250.645346	47.381364
2366.011025	251.794759	47.386369
2362.665290	253.101691	47.391373
2359.413548	236.529019	47.396378
2355.315427	249.265980	47.401383
2351.905049	244.130787	47.406388
2348.535375	248.385019	47.411393
2345.062545	247.812183	47.416397
2341.695036	240.869428	47.421402
2338.030996	243.427552	47.426407
2334.448193	245.246852	47.431412
2331.125939	235.394535	47.436417
2327.169980	236.983945	47.441421
2324.156865	245.276919	47.446426
2320.606315	228.273197	47.451431
2317.178725	234.453605	47.456436
2313.715927	237.213059	47.461441
2309.539461	241.935305	47.466445
2306.761931	230.810856	47.471450
2303.050461	234.254769	47.476455
2299.805100	226.013989	47.481460
2296.237700	235.804840	47.486465
2292.476191	240.301201	47.491469
2289.271129	238.174773	47.496474
2285.715084	248.393712	47.501479
2282.123659	238.136330	47.506484
2278.797144	233.142238	47.511489
2275.191814	243.019368	47.516493
2271.573960	234.888473	47.521498
2267.975900	252.261580	47.526503
2264.618692	234.794374	47.531508
2261.333461	248.450766	47.536513
2257.467791	235.297655	47.541517
2254.424873	234.396856	47.546522
2250.468203	248.002096	47.551527
2246.727429	237.120892	47.556532
2243.485666	234.213155	47.561537
2240.656941	238.091313	47.566541
2236.957188	231.988825	47.571546
2232.856812	236.457539	47.576551
2229.968020	236.699235	47.581556
2226.411767	229.576154	47.586561
2222.920132	227.548720	47.591565
2219.235416	232.789344	47.596570
2215.337903	237.948061	47.601575
2212.072545	231.132175	47.606580
2209.084956	241.581665	47.611585
2205.558269	240.614270	47.616589
2201.816838	226.984816	47.621594
2198.122114	239.677595	47.626599
2194.627115	228.972939	47.631604
2191.170492	231.698080	47.636609
2187.205743	237.943954	47.641613
2184.261742	234.024829	47.646618
2180.689245	228.462448	47.651623
2177.053769	227.207668	47.656628
2173.549689	228.431486	47.661633
2170.284630	231.006946	47.666637
2167.071619	227.650744	47.671642
2163.085922	235.004353	47.676647
2159.656253	224.720767	47.681652
2156.152334	237.441479	47.686657
2152.757993	227.235729	47.691661
2150.002185	224.185925	47.696666
2146.060101	241.998887	47.701671
2142.105043	228.531877	47.706676
2138.701863	220.046402	47.711681
2135.307722	225.394615	47.716685
2131.929365	225.772842	47.721690
2128.233936	235.304687	47.726695
2124.482670	228.723986	47.731700
2121.422864	231.270347	47.736705
2117.569569	234.327423	47.741709
2114.668662	227.699694	47.746714
2110.466124	227.645318	47.751719
2107.196852	227.993625	47.756724
2103.664840	216.719767	47.761729
2099.865814	233.493267	47.766733
2096.849750	219.847828	47.771738
2093.562083	221.850892	47.776743
2090.157956	219.701060	47.781748
2086.466326	221.408295	47.786753
2082.807648	222.970200	47.791757
2079.324073	226.455943	47.796762
2075.673195	219.081791	47.801767
2072.163096	224.936818	47.806772
2068.837465	224.976171	47.811777
2065.009602	218.117995	47.816781
2061.704267	217.204331	47.821786
2058.422423	226.204880	47.826791
2055.176110	224.046396	47.831796
2051.452393	220.414494	47.836801
2047.529045	217.709851	47.841805
2044.258734	207.228590	47.846810
2040.595429	215.275307	47.851815
2037.088212	218.208245	47.856820
2033.595412	215.005995	47.861825
2030.028195	232.942426	47.866829
2027.025350	217.034813	47.871834
2023.302033	216.358427	47.876839
2019.947954	221.477210	47.881844
2016.472981	217.750626	47.886849
2012.616020	225.719993	47.891853
2009.146448	214.542344	47.896858
2005.728397	219.086651	47.901863
2002.088633	224.146217	47.906868
1998.626208	216.874309	47.911873
1995.070892	219.407254	47.916877
1991.775128	207.852295	47.921882
1988.274051	214.921910	47.926887
1984.933152	213.557861	47.931892
1981.498245	209.505137	47.936897
1977.754918	210.853160	47.941901
1974.145959	209.242497	47.946906
1970.465839	206.973597	47.951911
1966.917191	205.878929	47.956916
1964.106227	209.792227	47.961921
1960.450517	217.447438	47.966925
1957.158880	206.797292	47.971930
1953.551807	210.572497	47.976935
1949.865509	207.491301	47.981940
1946.307491	211.084879	47.986945
1942.788777	210.280465	47.991949
1939.157848	205.719266	47.996954
1935.841736	216.316445	48.001959
1932.278832	211.754483	48.006964
1928.886279	204.658836	48.011969
1925.039679	216.127856	48.016973
1921.799044	207.276215	48.021978
1918.014759	222.634173	48.026983
1914.410542	213.131593	48.031988
1911.351747	214.196140	48.036993
1907.751657	218.276840	48.041997
1904.920851	214.533425	48.047002
1900.862730	208.481381	48.052007
1897.035607	204.733540	48.057012
1893.966935	204.953742	48.062017
1890.076196	212.389274	48.067021
1886.583797	205.493328	48.072026
1883.521442	208.365469	48.077031
1879.788634	218.022551	48.082036
1876.500351	210.120374	48.087041
1872.785425	216.070737	48.092045
1869.365266	208.617111	48.097050
1865.428573	199.656885	48.102055
1861.876505	206.566553	48.107060
1858.939186	195.727491	48.112065
1855.104278	215.512548	48.117069
1852.076885	209.245296	48.122074
1848.596405	205.700055	48.127079
1844.498511	200.945041	48.132084
1841.674148	204.781567	48.137089
1837.861483	199.323037	48.142093
1834.044010	197.917131	48.147098
1830.490067	205.854432	48.152103
1827.211610	195.603134	48.157108
1823.917141	196.614553	48.162113
1820.031613	209.997263	48.167117
1816.849181	192.230745	48.172122
1813.353082	197.968232	48.177127
1809.400890	200.326413	48.182132
1806.329137	199.502190	48.187137
1802.368605	205.456502	48.192141
1799.218074	197.956461	48.197146
1795.579901	201.110891	48.202151
1792.339134	203.373111	48.207156
1789.244770	201.294458	48.212161
1785.064222	203.381929	48.217165
1781.954281	199.284771	48.222170
1778.239412	199.606115	48.227175
1774.633908	198.309109	48.232180
1770.918359	204.708800	48.237185
1767.294916	202.279713	48.242189
1764.397432	193.637032	48.247194
1760.724575	207.580658	48.252199
1757.285426	204.400185	48.257204
1753.568337	207.414542	48.262209
1749.818837	198.833620	48.267213
1746.775098	194.355003	48.272218
1743.535595	202.068793	48.277223
1739.954289	198.396109	48.282228
1736.068836	199.532999	48.287233
1732.556719	189.699055	48.292237
1729.486572	188.119780	48.297242
1725.485027	195.048713	48.302247
1722.183252	205.131368	48.307252
1718.911169	187.420752	48.312257
1715.251376	206.619441	48.317261
1711.926926	195.696744	48.322266
1707.998532	199.253772	48.327271
1704.566960	204.990526	48.332276
1701.149632	197.092676	48.337281
1697.665690	200.323320	48.342285
1694.263944	192.579967	48.347290
1690.209460	186.848394	48.352295
1686.646859	185.018024	48.357300
1683.976879	181.672497	48.362305
1680.078349	189.789834	48.367309
1676.884484	192.329381	48.372314
1673.286163	194.975525	48.377319
1669.754784	198.693479	48.382324
1666.142906	192.761420	48.387329
1662.467840	186.879157	48.392333
1658.999989	185.753949	48.397338
1655.460379	197.255083	48.402343
1652.116706	203.088638	48.407348
1648.963468	194.062712	48.412353
1644.811340	195.743448	48.417357
1641.652811	189.548952	48.422362
1638.106281	194.628509	48.427367
1634.473400	192.733204	48.432372
1631.411273	182.802183	48.437377
1627.347405	196.808988	48.442381
1624.435848	182.478503	48.447386
1620.603279	197.723165	48.452391
1617.159386	199.143995	48.457396
1613.720537	192.011475	48.462401
1609.965999	192.108695	48.467405
1606.615461	186.473418	48.472410
1603.209364	196.728215	48.477415
1599.530398	191.256153	48.482420
1596.254323	193.129657	48.487425
1592.455582	184.300163	48.492429
1589.252942	191.930872	48.497434
1585.339615	195.449566	48.502439
1582.164527	192.523060	48.507444
1578.534809	184.234338	48.512449
1575.047175	184.473301	48.517453
1571.598114	184.394641	48.522458
1568.186763	188.771882	48.527463
1564.301853	182.226215	48.532468
1560.737373	184.476149	48.537473
1557.114912	187.072958	48.542477
1554.491072	192.407144	48.547482
1551.021976	192.538484	48.552487
1547.307410	186.658465	48.557492
1543.693383	185.572434	48.562497
1539.819628	188.263799	48.567501
1536.208727	188.172204	48.572506
1532.672659	195.611320	48.577511
1529.615057	185.666581	48.582516
1526.232584	178.390543	48.587521
1522.799377	187.244382	48.592525
1519.244041	184.993019	48.597530
1515.515605	184.013096	48.602535
1511.472979	179.329976	48.607540
1508.238340	170.394822	48.612545
1504.919871	188.016144	48.617549
1501.480031	181.439291	48.622554
1498.465267	184.622091	48.627559
1494.975294	190.180034	48.632564
1491.360127	178.725753	48.637569
1487.572120	181.820112	48.642573
1483.812578	181.256736	48.647578
1480.335390	178.875985	48.652583
1477.098630	175.889369	48.657588
1473.795133	177.105667	48.662593
1469.558109	182.052119	48.667597
1466.308380	176.026081	48.672602
1463.058148	180.929842	48.677607
1459.130323	180.242026	48.682612
1456.062492	174.752655	48.687617
1452.358932	182.386565	48.692621
1449.299585	173.891128	48.697626
1445.774447	179.497217	48.702631
1441.860779	176.064041	48.707636
1438.538073	176.237771	48.712641
1434.849021	186.695693	48.717645
1431.558021	176.428552	48.722650
1428.052702	172.216878	48.727655
1424.423521	184.985509	48.732660
1421.104568	173.023738	48.737665
1417.563313	183.727096	48.742669
1413.747451	186.457708	48.747674
1410.322688	176.360739	48.752679
1406.428944	176.342234	48.757684
1403.543735	179.341301	48.762689
1400.038117	180.939050	48.767693
1396.609239	179.887158	48.772698
1393.096630	173.702107	48.777703
1389.291348	183.469202	48.782708
1386.387595	180.766453	48.787713
1382.558199	169.899588	48.792717
1378.781582	179.161078	48.797722
1375.028203	175.654625	48.802727
1371.887438	180.886836	48.807732
1368.578917	177.628087	48.812737
1365.083719	180.216909	48.817741
1361.762235	169.912817	48.822746
1357.783644	175.856309	48.827751
1354.236210	171.565501	48.832756
1351.066013	176.734010	48.837761
1346.905535	191.269789	48.842765
1343.697151	177.462207	48.847770
1340.334746	172.106558	48.852775
1337.038210	179.843419	48.857780
1333.464018	174.170922	48.862785
1330.000970	179.591699	48.867789
1326.380520	184.236781	48.872794
1322.815233	172.157978	48.877799
1319.204608	186.746650	48.882804
1315.913833	180.498091	48.887809
1312.161991	174.467112	48.892813
1308.732515	180.833203	48.897818
1305.250369	183.283260	48.902823
1301.842980	181.153703	48.907828
1298.343262	177.643408	48.912833
1294.972921	186.518431	48.917837
1291.262224	170.319115	48.922842
1287.904535	176.172982	48.927847
1284.510570	177.561162	48.932852
1281.158657	173.284884	48.937857
1277.492319	173.509393	48.942861
1274.107815	172.980317	48.947866
1270.556740	168.403957	48.952871
1266.670155	182.112310	48.957876
1263.166541	171.485545	48.962881
1259.615556	170.240093	48.967885
1256.094018	181.502005	48.972890
1252.826432	167.998847	48.977895
1249.310859	164.868458	48.982900
1246.166425	165.801803	48.987905
1242.345969	172.479492	48.992909
1238.457179	166.613626	48.997914
1235.194541	171.868570	49.002919
1231.384386	165.866705	49.007924
1228.362416	160.002490	49.012929
1224.858706	167.884773	49.017933
1221.409546	160.936312	49.022938
1217.999196	171.776377	49.027943
1214.393454	171.350937	49.032948
1211.126062	171.023056	49.037953
1207.271528	177.964966	49.042957
1203.644468	173.209892	49.047962
1200.410693	176.428272	49.052967
1196.535443	167.444056	49.057972
1193.411616	164.638522	49.062977
1189.659009	170.922054	49.067981
1185.822690	173.504132	49.072986
1182.780022	163.453051	49.077991
1179.276931	179.550910	49.082996
1175.942696	169.653916	49.088001
1172.169568	170.795555	49.093005
1168.697204	170.997374	49.098010
1165.327633	167.205909	49.103015
1161.823203	165.401930	49.108020
1158.561022	171.830439	49.113025
1154.514126	170.824559	49.118029
1151.021939	167.452207	49.123034
1147.488954	177.383014	49.128039
1144.154578	171.012708	49.133044
1141.121815	152.581888	49.138049
1137.365095	171.421431	49.143053
1133.720014	160.461370	49.148058
1130.108644	163.403232	49.153063
1126.324028	171.823435	49.158068
1122.598121	163.597843	49.163073
1119.348154	164.510290	49.168077
1116.664252	163.988163	49.173082
1113.242894	162.410920	49.178087
1109.326686	172.717348	49.183092
1105.654662	162.086428	49.188097
1102.176588	163.478320	49.193101
1098.887864	161.395775	49.198106
1095.201332	171.140628	49.203111
1091.506223	173.477271	49.208116
1088.333098	163.577610	49.213121
1084.524149	169.169348	49.218125
1081.199021	175.669547	49.223130
1077.721538	163.048114	49.228135
1073.742879	163.116624	49.233140
1070.233645	163.262625	49.238145
1066.766460	171.325012	49.243149
1063.754538	168.121144	49.248154
1060.391842	159.242019	49.253159
1056.596190	169.562306	49.258164
1053.321679	160.007239	49.263169
1049.536211	166.063237	49.268173
1046.031648	165.244122	49.273178
1042.570251	161.546216	49.278183
1039.210747	169.833825	49.283188
1035.920674	160.612129	49.288193
1031.911120	165.548396	49.293197
1028.683996	160.731444	49.298202
1024.804824	163.812972	49.303207
1021.180911	171.318397	49.308212
1018.222666	150.767776	49.313217
1014.636382	166.848634	49.318221
1011.080088	159.070829	49.323226
1007.601225	168.631179	49.328231
1004.076256	164.995880	49.333236
1000.994624	162.140263	49.338241
997.294719	169.713197	49.343245
993.532595	164.074988	49.348250
990.081147	154.810908	49.353255
986.382749	160.282923	49.358260
983.312247	154.376928	49.363265
979.885354	160.637067	49.368269
976.439135	157.843237	49.373274
972.725074	153.382653	49.378279
969.011844	150.113692	49.383284
965.270553	154.020034	49.388289
961.841494	162.721964	49.393293
958.267280	152.340283	49.398298
954.908227	157.526614	49.403303
951.432592	163.937075	49.408308
948.296665	146.002295	49.413313
944.750802	163.747129	49.418317
940.932876	157.598847	49.423322
937.554671	149.930693	49.428327
933.947978	160.723268	49.433332
930.455527	160.514864	49.438337
926.592902	161.705350	49.443341
923.633135	152.447734	49.448346
919.960105	161.126332	49.453351
916.579240	153.272465	49.458356
913.446361	157.538405	49.463361
909.419922	161.049588	49.468365
905.797075	164.307181	49.473370
902.417049	155.190690	49.478375
898.704859	161.495802	49.483380
895.665827	148.464603	49.488385
892.222401	167.385682	49.493389
888.549483	156.383125	49.498394
884.928721	152.627076	49.503399
881.314944	164.841384	49.508404
878.069570	159.354695	49.513409
874.551614	166.106819	49.518413
870.692954	168.520108	49.523418
867.626639	158.020085	49.528423
863.721115	161.674109	49.533428
860.146692	159.915295	49.538433
857.130766	159.808387	49.543437
853.269151	167.031324	49.548442
849.996607	159.699547	49.553447
846.323789	168.757773	49.558452
843.290619	158.496265	49.563457
839.661030	158.912253	49.568461
835.719159	166.106917	49.573466
832.912981	162.496861	49.578471
829.090018	164.822887	49.583476
825.394504	168.113239	49.588481
821.658771	161.278235	49.593485
817.977422	172.906375	49.598490
814.800504	158.490469	49.603495
811.477754	156.569368	49.608500
808.251655	157.240754	49.613505
804.186866	153.236952	49.618509
800.621913	164.497916	49.623514
797.733304	153.444831	49.628519
793.859670	160.601215	49.633524
790.573697	154.320989	49.638529
786.646608	157.725367	49.643533
783.500837	151.432057	49.648538
779.948042	156.150277	49.653543
776.440796	151.399057	49.658548
772.725258	147.342930	49.663553
769.387800	168.586255	49.668557
765.867351	164.883455	49.673562
762.830710	154.107787	49.678567
758.911299	149.947711	49.683572
755.241920	143.813597	49.688577
751.610205	157.823577	49.693581
748.214483	153.272279	49.698586
744.805038	159.173693	49.703591
741.289582	161.658922	49.708596
737.962957	150.685804	49.713601
734.242453	147.835297	49.718605
730.593955	146.495150	49.723610
727.417005	146.727729	49.728615
723.646530	162.276968	49.733620
720.448136	156.488222	49.738625
717.121696	153.862495	49.743629
713.551261	148.955809	49.748634
709.924619	141.646096	49.753639
706.041561	150.106421	49.758644
702.998795	145.685194	49.763649
699.094577	154.806259	49.768653
695.562940	165.368615	49.773658
692.487517	153.381987	49.778663
688.633181	152.463078	49.783668
685.009226	155.028406	49.788673
681.444558	162.923359	49.793677
678.092188	162.173224	49.798682
675.272316	154.862879	49.803687
671.416628	166.198945	49.808692
667.797309	154.411073	49.813697
664.374431	157.340488	49.818701
660.701095	152.809142	49.823706
657.287818	153.279575	49.828711
653.657209	158.399903	49.833716
650.511640	152.680409	49.838721
646.776337	153.229683	49.843725
643.220804	158.732631	49.848730
639.736690	149.552695	49.853735
635.986744	147.758969	49.858740
632.776256	156.135679	49.863745
629.216397	155.140349	49.868749
625.514825	161.124397	49.873754
622.391204	145.066392	49.878759
618.757269	147.973466	49.883764
615.385367	145.251518	49.888769
611.572905	149.416534	49.893773
608.190732	158.775210	49.898778
605.073411	149.047064	49.903783
601.132649	152.163856	49.908788
597.742153	148.441371	49.913793
594.051863	144.757059	49.918797
590.310425	152.737083	49.923802
587.150961	152.146525	49.928807
583.415520	151.101297	49.933812
580.207436	143.013698	49.938817
576.851147	150.976284	49.943821
573.005140	147.390906	49.948826
570.262314	143.681625	49.953831
566.238676	149.370148	49.958836
562.944269	141.952774	49.963841
559.347235	154.675277	49.968845
555.342563	149.015456	49.973850
552.078863	145.439472	49.978855
548.354335	145.842492	49.983860
544.944080	148.904740	49.988865
541.628306	152.975325	49.993869
538.340510	150.041525	49.998874
534.977018	146.874877	50.003879
530.730367	154.184655	50.008884
527.587953	157.305372	50.013889
524.432150	158.020531	50.018893
520.447581	160.169599	50.023898
517.197105	148.453502	50.028903
513.851348	163.464557	50.033908
510.204771	148.204896	50.038913
506.799361	152.113512	50.043917
503.390256	154.023007	50.048922
499.805063	151.621662	50.053927
495.867531	149.111496	50.058932
492.235160	145.296037	50.063937
488.744608	153.808446	50.068941
485.490921	153.790803	50.073946
482.332048	139.304865	50.078951
478.605905	152.430026	50.083956
475.423036	137.607796	50.088961
471.463186	153.392231	50.093965
467.429423	151.254320	50.098970
464.404540	142.067799	50.103975
460.919550	143.959562	50.108980
457.933633	150.305135	50.113985
453.909443	141.995682	50.118989
450.260063	151.168890	50.123994
447.118715	145.414086	50.128999
443.460258	155.891240	50.134004
440.049658	153.126353	50.139009
436.869757	147.705850	50.144013
432.910358	141.369264	50.149018
429.661209	150.807847	50.154023
425.857764	146.816571	50.159028
422.623473	147.089353	50.164033
419.114458	154.749901	50.169037
415.219633	150.898030	50.174042
411.922111	144.520191	50.179047
408.558577	156.663952	50.184052
405.265921	141.662985	50.189057
401.861245	147.411244	50.194061
397.803028	156.082482	50.199066
394.355876	146.747629	50.204071
390.761527	155.378449	50.209076
387.482805	149.751535	50.214081
384.418962	156.510550	50.219085
380.651427	152.504489	50.224090
377.054062	147.222337	50.229095
373.586965	149.822195	50.234100
369.811797	155.975586	50.239105
366.270100	151.627975	50.244109
362.691604	155.389946	50.249114
359.485154	154.367065	50.254119
355.880677	149.950908	50.259124
352.811848	166.071520	50.264129
349.097749	155.537640	50.269133
345.623083	152.344277	50.274138
342.252614	151.303417	50.279143
337.998370	155.933323	50.284148
334.757713	148.786590	50.289153
331.747321	153.363433	50.294157
327.918340	153.347090	50.299162
324.167038	150.963719	50.304167
320.604485	155.119966	50.309172
317.533874	148.129734	50.314177
314.324858	149.860062	50.319181
310.347515	154.611952	50.324186
306.998665	147.168599	50.329191
303.512951	151.906159	50.334196
299.661134	137.776228	50.339201
296.920083	147.852678	50.344205
292.875381	149.062165	50.349210
289.547386	145.136265	50.354215
285.433255	147.682060	50.359220
282.242669	148.500354	50.364225
279.098479	146.709660	50.369229
275.454097	159.808484	50.374234
272.270992	150.213437	50.379239
268.257743	158.779649	50.384244
264.752592	156.832937	50.389249
261.476753	145.496772	50.394253
257.581096	158.375880	50.399258
254.188858	143.112570	50.404263
250.766739	147.280671	50.409268
247.600792	141.048706	50.414273
244.004615	157.225196	50.419277
240.222626	155.579062	50.424282
236.775007	134.265853	50.429287
233.350306	152.798293	50.434292
229.787608	151.206894	50.439297
226.613180	143.357124	50.444301
222.840947	153.128952	50.449306
219.576222	157.068824	50.454311
215.731846	151.326713	50.459316
212.217862	157.978450	50.464321
208.996660	154.882292	50.469325
204.862755	147.072280	50.474330
201.520569	151.694921	50.479335
198.484958	143.565039	50.484340
195.159450	151.284257	50.489345
191.637916	147.118891	50.494349
187.719300	155.069196	50.499354
184.624422	148.737226	50.504359
180.621406	147.292599	50.509364
177.297690	143.535445	50.514369
173.922076	146.631221	50.519373
170.313612	145.173204	50.524378
166.675006	151.881363	50.529383
163.182600	154.250910	50.534388
159.604598	143.636872	50.539393
156.439232	152.355160	50.544397
152.980352	148.580298	50.549402
149.591946	147.293896	50.554407
145.753814	153.351852	50.559412
141.876541	153.544658	50.564417
139.007840	150.361684	50.569421
135.131846	145.647111	50.574426
131.733507	146.180266	50.579431
128.143214	156.784812	50.584436
124.695329	147.779659	50.589441
121.321860	143.751664	50.594445
117.634380	157.111415	50.599450
114.279846	147.970287	50.604455
110.855818	154.607207	50.609460
107.088728	148.752857	50.614465
103.741005	133.284800	50.619469
100.166958	154.084377	50.624474
96.837747	142.936295	50.629479
93.134486	146.443578	50.634484
89.975067	149.289197	50.639489
86.242053	150.741496	50.644493
82.516188	141.004517	50.649498
79.335805	148.711643	50.654503
75.819794	158.665053	50.659508
72.107344	148.625555	50.664513
68.835705	145.946041	50.669517
65.174026	151.040822	50.674522
61.470866	141.034824	50.679527
58.137817	151.563446	50.684532
54.826832	146.196782	50.689537
51.196318	148.038324	50.694541
47.597321	155.190553	50.699546
43.947713	145.563723	50.704551
40.493477	143.958063	50.709556
37.078788	144.920058	50.714561
33.748788	135.074391	50.719565
30.161674	156.449731	50.724570
26.811204	137.676663	50.729575
23.266499	146.517374	50.734580
19.376271	149.112558	50.739585
16.077142	144.995882	50.744589
12.206748	143.537243	50.749594
9.072670	148.637698	50.754599
5.556391	150.149133	50.759604
2.371066	145.443436	50.764609