Thu Jun 16 11:10:34 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.648766	89.789208	0.000000
0.498675	81.846763	0.005005
0.616980	82.088477	0.010010
0.571934	81.308694	0.015014
0.606855	73.074444	0.020019
0.508135	81.972285	0.025024
0.631669	89.644526	0.030029
0.895993	68.071377	0.035034
0.497417	64.956877	0.040038
0.196333	39.188240	0.045043
-0.395475	40.189043	0.050048
-0.780294	31.427031	0.055053
-1.338878	29.909838	0.060058
-1.705104	15.848950	0.065062
-1.502321	19.867358	0.070067
-2.134960	6.780015	0.075072
-2.580425	5.632234	0.080077
-2.628384	11.827328	0.085082
-3.204715	12.580222	0.090086
-3.351591	10.007772	0.095091
-4.068720	13.161182	0.100096
-4.490720	12.610420	0.105101
-3.949282	9.338912	0.110106
-4.404366	8.700390	0.115110
-4.586481	0.191289	0.120115
-4.617333	18.047627	0.125120
-4.620092	14.288829	0.130125
-4.767544	6.832249	0.135130
-5.613676	13.550998	0.140134
-5.966319	10.268114	0.145139
-6.205382	11.446011	0.150144
-6.611045	19.893381	0.155149
-6.135392	7.060415	0.160154
-6.512665	4.477700	0.165158
-7.290570	23.614209	0.170163
-7.905078	19.229529	0.175168
-8.023861	15.515554	0.180173
-7.699367	11.660947	0.185178
-7.807861	18.903287	0.190182
-7.702756	19.467114	0.195187
-8.322163	21.866845	0.200192
-9.400730	18.737465	0.205197
-9.322252	19.504578	0.210202
-9.941242	32.314834	0.215206
-9.368718	14.539498	0.220211
-9.581612	20.691018	0.225216
-9.513547	17.566103	0.230221
-9.935955	12.057982	0.235226
-10.595472	20.870788	0.240230
-10.615936	20.910010	0.245235
-11.368485	15.569602	0.250240
-11.283320	24.114621	0.255245
-11.241931	17.589785	0.260250
-12.170977	12.299262	0.265254
-12.472383	20.636374	0.270259
-12.688684	19.802618	0.275264
-12.784784	16.266516	0.280269
-12.787674	17.982900	0.285274
-12.739560	19.819204	0.290278
-12.684053	5.655584	0.295283
-13.545397	17.571830	0.300288
-14.068949	17.728621	0.305293
-14.202696	9.350525	0.310298
-14.837098	10.358564	0.315302
-14.265073	16.502107	0.320307
-14.632383	16.120180	0.325312
-15.207315	12.098124	0.330317
-15.834210	12.773152	0.335322
-15.880522	17.116746	0.340326
-15.852659	17.810932	0.345331
-15.893330	20.165139	0.350336
-16.320464	26.957403	0.355341
-15.774022	5.973839	0.360346
-16.367531	20.989412	0.365350
-17.034408	9.969386	0.370355
-17.155743	3.097058	0.375360
-17.613423	23.555971	0.380365
-17.844041	18.358974	0.385370
-18.396711	13.563052	0.390374
-18.459488	22.707273	0.395379
-18.560264	17.786654	0.400384
-18.918493	7.017897	0.405389
-18.502774	13.624500	0.410394
-19.122599	20.235021	0.415398
-19.645085	12.087396	0.420403
-20.239464	19.966437	0.425408
-20.752595	11.882378	0.430413
-20.291227	10.401143	0.435418
-20.727132	17.228000	0.440422
-20.760796	9.926542	0.445427
-20.575723	19.956649	0.450432
-21.289687	11.068509	0.455437
-21.814451	14.057738	0.460442
-21.935189	27.233240	0.465446
-22.005522	10.568241	0.470451
-21.831925	21.834201	0.475456
-22.671100	12.703052	0.480461
-23.122815	6.237119	0.485466
-23.719950	21.028460	0.490470
-23.111457	13.605785	0.495475
-23.115971	18.263292	0.500480
-23.803503	22.430804	0.505485
-23.596421	10.621157	0.510490
-24.625355	17.505569	0.515494
-24.744250	13.179866	0.520499
-25.234846	13.665449	0.525504
-25.346833	18.542068	0.530509
-24.959511	13.305500	0.535514
-25.195560	17.310795	0.540518
-25.527012	13.963246	0.545523
-26.355484	10.229428	0.550528
-26.857496	8.032050	0.555533
-26.715848	21.485794	0.560538
-27.197302	26.517490	0.565542
-27.055087	5.852296	0.570547
-27.054172	13.156856	0.575552
-27.314438	18.843358	0.580557
-27.745889	14.631360	0.585562
-28.342313	15.738881	0.590566
-28.639979	16.053480	0.595571
-28.584876	15.607271	0.600576
-28.843591	11.431741	0.605581
-28.525028	17.781328	0.610586
-29.495491	17.826114	0.615590
-29.886007	4.205402	0.620595
-29.947272	8.186250	0.625600
-30.061634	9.949664	0.630605
-29.963283	10.652918	0.635610
-30.349321	17.591595	0.640614
-31.072932	15.707757	0.645619
-31.575904	3.953308	0.650624
-31.652761	13.811040	0.655629
-31.910445	15.274656	0.660634
-31.872974	19.316632	0.665638
-31.903694	13.313556	0.670643
-32.032120	17.201623	0.675648
-32.602027	5.815655	0.680653
-32.983441	13.912544	0.685658
-33.206394	13.122803	0.690662
-33.241443	8.403332	0.695667
-33.781643	10.692109	0.700672
-33.837184	17.195070	0.705677
-33.603983	5.766056	0.710682
-34.664276	16.445711	0.715686
-34.978279	9.552048	0.720691
-35.074254	11.442942	0.725696
-34.869720	18.664034	0.730701
-35.225431	17.084118	0.735706
-35.273220	10.083224	0.740710
-35.883810	-0.404880	0.745715
-36.561316	13.592949	0.750720
-36.718744	13.781576	0.755725
-36.622471	16.666792	0.760730
-36.718191	19.612150	0.765734
-36.804605	18.370308	0.770739
-37.111006	13.395379	0.775744
-37.902011	21.252162	0.780749
-37.912332	16.641165	0.785754
-38.108818	13.493184	0.790758
-38.380157	27.347544	0.795763
-38.441900	23.423088	0.800768
-38.805057	17.946611	0.805773
-39.625345	12.944143	0.810778
-39.943114	12.410489	0.815782
-40.140996	11.062766	0.820787
-40.206697	12.975590	0.825792
-40.208056	17.169594	0.830797
-40.056147	7.864701	0.835802
-40.562741	7.394020	0.840806
-40.146525	7.571306	0.845811
-40.877541	21.767894	0.850816
-41.610443	21.398243	0.855821
-41.671263	7.922620	0.860826
-41.882794	16.066115	0.865830
-41.738772	6.237987	0.870835
-42.361775	6.440319	0.875840
-43.040548	18.077788	0.880845
-43.251556	17.917356	0.885850
-43.301668	7.883851	0.890854
-43.249265	15.518874	0.895859
-43.190389	12.865858	0.900864
-43.621715	25.634834	0.905869
-43.815196	15.386179	0.910874
-44.420018	20.029935	0.915878
-44.412694	13.625269	0.920883
-44.491237	18.530889	0.925888
-45.001367	8.889690	0.930893
-45.726628	11.039269	0.935898
-45.979775	17.813627	0.940902
-46.114178	7.589545	0.945907
-46.123757	16.084905	0.950912
-46.284843	10.318539	0.955917
-46.248367	15.223401	0.960922
-47.218335	10.353696	0.965926
-47.442656	7.348233	0.970931
-48.029260	14.625485	0.975936
-47.785689	27.746598	0.980941
-47.703187	8.160380	0.985946
-48.240951	14.823040	0.990950
-48.061594	20.355599	0.995955
-48.246457	8.889524	1.000960
-49.011817	10.583145	1.005965
-49.345684	10.966175	1.010970
-49.566715	13.852134	1.015974
-49.828129	13.175000	1.020979
-49.505457	19.154943	1.025984
-50.070348	18.964700	1.030989
-50.353469	12.327464	1.035994
-51.092968	24.415066	1.040998
-50.992150	9.530498	1.046003
-51.003618	10.014837	1.051008
-51.468113	14.234869	1.056013
-51.334422	11.574521	1.061018
-52.121119	15.722709	1.066022
-52.445422	11.534245	1.071027
-52.696473	14.986897	1.076032
-52.870698	11.071859	1.081037
-52.579068	13.556121	1.086042
-52.812033	15.346437	1.091046
-52.768885	14.295979	1.096051
-53.809710	19.958961	1.101056
-54.498436	25.323338	1.106061
-54.237578	11.439006	1.111066
-54.766264	15.088086	1.116070
-54.706619	8.706739	1.121075
-54.350124	10.908886	1.126080
-55.296290	13.850954	1.131085
-55.570958	-2.702418	1.136090
-55.739314	15.189457	1.141094
-56.363600	22.690075	1.146099
-56.275620	3.911423	1.151104
-56.184577	16.783082	1.156109
-56.247010	11.035829	1.161114
-56.611217	8.328629	1.166118
-57.160545	9.532744	1.171123
-57.648140	12.967269	1.176128
-57.703582	14.855016	1.181133
-57.671281	11.053432	1.186138
-57.981058	13.330471	1.191142
-58.762472	10.638750	1.196147
-59.225286	9.626036	1.201152
-59.480421	12.727467	1.206157
-59.464467	8.275402	1.211162
-59.518753	19.761327	1.216166
-59.579015	9.927892	1.221171
-59.339087	12.714882	1.226176
-59.709732	16.256554	1.231181
-60.580310	9.269803	1.236186
-61.061768	15.091117	1.241190
-61.099592	12.506073	1.246195
-60.823649	15.077868	1.251200
-61.139147	15.319551	1.256205
-61.746071	14.927407	1.261210
-62.173709	10.189456	1.266214
-62.616142	19.555246	1.271219
-62.488436	13.959965	1.276224
-62.702483	21.317316	1.281229
-62.863079	14.512641	1.286234
-62.726106	11.501926	1.291238
-63.143166	13.440064	1.296243
-64.020698	17.336507	1.301248
-64.133123	20.357924	1.306253
-64.213918	4.228778	1.311258
-64.341473	5.873818	1.316262
-64.473111	10.829545	1.321267
-64.849264	6.745642	1.326272
-65.461831	20.039212	1.331277
-65.663213	15.887257	1.336282
-65.844037	10.639519	1.341286
-65.998941	6.086456	1.346291
-65.750700	16.087174	1.351296
-66.023372	16.679299	1.356301
-67.098188	6.824814	1.361306
-67.660126	11.841888	1.366310
-67.448186	12.895234	1.371315
-67.268506	7.836918	1.376320
-67.694762	8.059319	1.381325
-67.676368	7.903101	1.386330
-67.810580	19.957651	1.391334
-68.146486	8.939073	1.396339
-68.355998	15.190755	1.401344
-69.042294	13.605495	1.406349
-68.982290	17.223482	1.411354
-69.637083	17.148232	1.416358
-69.961446	19.977181	1.421363
-70.164808	8.920223	1.426368
-70.534243	17.377092	1.431373
-70.386146	9.971510	1.436378
-70.503616	9.453491	1.441382
-70.522661	18.383108	1.446387
-71.313045	13.704909	1.451392
-71.975820	11.029197	1.456397
-71.721301	17.579073	1.461402
-72.166806	18.209331	1.466406
-72.357049	12.217923	1.471411
-72.503737	14.088293	1.476416
-72.512384	12.059961	1.481421
-72.729313	12.932816	1.486426
-73.127169	15.545133	1.491430
-73.906866	25.065220	1.496435
-74.001575	18.196580	1.501440
-74.033950	18.551587	1.506445
-74.005109	13.115595	1.511450
-74.104939	23.917884	1.516454
-74.786780	14.978669	1.521459
-75.209707	16.259760	1.526464
-75.718476	23.241215	1.531469
-75.589310	12.221738	1.536474
-75.913170	13.345974	1.541478
-75.720769	19.052371	1.546483
-75.565543	13.308411	1.551488
-76.268009	22.199939	1.556493
-76.964661	18.451741	1.561498
-77.340403	21.140808	1.566502
-77.547728	18.661022	1.571507
-77.387419	15.123587	1.576512
-77.622012	17.832240	1.581517
-77.048317	20.643584	1.586522
-78.245679	18.178946	1.591526
-78.785843	14.556912	1.596531
-78.580070	14.383537	1.601536
-78.945392	23.989138	1.606541
-79.102954	14.210159	1.611546
-79.917666	17.999542	1.616550
-80.347556	19.621151	1.621555
-80.432180	15.060912	1.626560
-80.414616	28.947432	1.631565
-80.380328	12.060052	1.636570
-80.564447	17.585397	1.641574
-80.563334	27.943145	1.646579
-80.982196	15.735395	1.651584
-81.870170	10.975463	1.656589
-81.665216	7.562157	1.661594
-81.865910	19.341795	1.666598
-81.990520	13.667858	1.671603
-81.841007	14.970853	1.676608
-83.003118	25.963501	1.681613
-83.317567	14.767745	1.686618
-84.120158	22.601684	1.691622
-84.068488	15.182343	1.696627
-83.695323	8.496039	1.701632
-83.864452	19.446411	1.706637
-83.908133	14.235989	1.711642
-84.001482	18.424083	1.716646
-84.454845	25.893890	1.721651
-84.910774	11.680039	1.726656
-85.597330	21.139448	1.731661
-85.565661	15.571878	1.736666
-85.856998	27.230657	1.741670
-85.630895	21.177541	1.746675
-85.995790	21.206406	1.751680
-86.994515	15.818105	1.756685
-86.766451	20.857533	1.761690
-87.053366	24.860483	1.766694
-87.429003	21.669305	1.771699
-87.176898	15.218267	1.776704
-87.579932	30.522100	1.781709
-87.938561	11.794071	1.786714
-88.363423	30.122371	1.791718
-88.677679	24.086344	1.796723
-88.727493	8.989416	1.801728
-88.955363	21.356390	1.806733
-89.188909	13.232844	1.811738
-89.728495	22.853531	1.816742
-90.201509	20.480991	1.821747
-90.326689	10.885388	1.826752
-90.680992	16.940707	1.831757
-90.479839	16.712356	1.836762
-90.990182	24.229857	1.841766
-90.852617	18.370134	1.846771
-90.582290	11.793954	1.851776
-91.495783	30.431983	1.856781
-91.902784	22.351108	1.861786
-92.174887	17.031049	1.866790
-92.358581	14.898071	1.871795
-92.334023	11.790708	1.876800
-92.602448	15.923289	1.881805
-92.918470	18.647866	1.886810
-93.312344	17.215040	1.891814
-93.932986	14.447821	1.896819
-94.016676	9.442898	1.901824
-94.185607	11.476960	1.906829
-93.841309	14.292178	1.911834
-94.048009	5.780932	1.916838
-95.155177	-0.495667	1.921843
-95.360495	18.951365	1.926848
-95.527036	14.488915	1.931853
-95.674708	11.487756	1.936858
-95.508696	21.659710	1.941862
-95.751920	12.229919	1.946867
-95.514784	17.252653	1.951872
-96.432684	19.590736	1.956877
-96.779543	11.189467	1.961882
-96.949928	15.751560	1.966886
-97.038216	18.035204	1.971891
-97.808408	18.753851	1.976896
-98.477449	23.172838	1.981901
-98.390528	13.801638	1.986906
-98.539588	26.970959	1.991910
-98.487515	7.747300	1.996915
-98.790711	18.018960	2.006912
-98.487920	15.134893	2.016909
-97.415799	14.867033	2.026906
-97.326843	15.905231	2.036902
-97.159686	17.844858	2.046899
-96.938967	21.208431	2.056896
-96.106618	15.518134	2.066893
-95.601670	13.137819	2.076890
-94.714293	17.063802	2.086886
-94.708451	4.640336	2.096883
-94.255631	14.190532	2.106880
-93.217749	7.264617	2.116877
-93.027007	18.607317	2.126874
-92.524903	17.027735	2.136870
-91.675230	16.329412	2.146867
-91.460958	21.790795	2.156864
-91.346801	18.739108	2.166861
-90.626157	11.413754	2.176858
-90.021996	8.856083	2.186854
-89.328964	15.526621	2.196851
-88.792999	15.314035	2.206848
-88.336569	15.738336	2.216845
-88.148573	20.685567	2.226842
-87.660886	22.887625	2.236838
-87.425340	21.890593	2.246835
-85.832088	21.010854	2.256832
-85.659938	10.920284	2.266829
-85.393918	21.211385	2.276826
-85.468284	21.480956	2.286822
-84.411045	16.998856	2.296819
-83.903457	13.230846	2.306816
-83.596839	16.751456	2.316813
-82.850500	8.795644	2.326810
-82.111237	16.527141	2.336806
-82.008755	22.692036	2.346803
-81.665866	20.557696	2.356800
-80.496965	20.261991	2.366797
-80.546051	18.076959	2.376794
-80.217385	20.372715	2.386790
-79.235792	12.433733	2.396787
-78.746273	18.779043	2.406784
-78.942504	18.666129	2.416781
-77.791712	13.025986	2.426778
-77.447330	15.844602	2.436774
-77.241668	23.655844	2.446771
-76.116342	15.162858	2.456768
-75.629101	17.450878	2.466765
-75.616314	17.391482	2.476762
-75.195794	20.579052	2.486758
-74.176552	11.659240	2.496755
-74.041265	13.263691	2.506752
-73.643447	25.244223	2.516749
-73.081523	15.704085	2.526746
-72.255077	17.213228	2.536742
-71.682184	20.352403	2.546739
-71.462139	15.985846	2.556736
-71.196094	14.908406	2.566733
-70.355583	21.051592	2.576730
-69.681496	19.734988	2.586726
-69.439722	18.462518	2.596723
-69.311051	14.409179	2.606720
-68.253838	14.917874	2.616717
-67.809063	12.916447	2.626714
-67.620138	17.931782	2.636710
-66.683096	17.579224	2.646707
-66.441336	18.094222	2.656704
-66.211910	13.769134	2.666701
-65.243458	10.336081	2.676698
-64.853071	13.918859	2.686694
-64.460833	16.619280	2.696691
-63.577998	11.667615	2.706688
-63.366399	19.151705	2.716685
-63.187585	10.841620	2.726682
-62.496478	20.595739	2.736678
-61.866739	10.807277	2.746675
-61.649703	14.538376	2.756672
-60.266446	13.974573	2.766669
-60.078253	21.712841	2.776666
-60.109025	21.704699	2.786662
-59.824097	20.537360	2.796659
-58.762680	12.365107	2.806656
-58.377574	19.009395	2.816653
-58.065748	17.429651	2.826650
-57.291426	15.425919	2.836646
-56.920653	14.979462	2.846643
-56.223652	19.683342	2.856640
-55.636547	15.618645	2.866637
-55.280793	15.361413	2.876634
-55.287988	19.967962	2.886630
-54.320341	19.127710	2.896627
-53.790385	18.421530	2.906624
-53.349842	22.407094	2.916621
-53.075742	16.052258	2.926618
-52.297593	19.330180	2.936614
-52.009457	12.520764	2.946611
-50.838361	20.093680	2.956608
-50.754330	15.022287	2.966605
-50.395559	17.093186	2.976602
-50.251477	13.724263	2.986598
-49.038212	19.054335	2.996595
-48.937799	14.456056	3.006592
-48.827261	15.649873	3.016589
-47.472617	21.616626	3.026586
-46.806710	17.622375	3.036582
-47.114228	17.660265	3.046579
-46.791220	16.779762	3.056576
-45.745190	12.191900	3.066573
-45.570377	13.013313	3.076570
-44.858967	15.968046	3.086566
-44.342358	21.440266	3.096563
-44.234269	16.742432	3.106560
-43.202137	18.987920	3.116557
-42.900879	19.055789	3.126554
-42.199756	20.963974	3.136550
-41.484450	24.599544	3.146547
-41.166044	19.661688	3.156544
-40.920468	23.574224	3.166541
-40.712798	18.645631	3.176538
-39.658484	16.290794	3.186534
-39.533600	15.446935	3.196531
-38.971550	26.537839	3.206528
-38.259061	21.174310	3.216525
-38.042388	21.659624	3.226522
-37.219565	25.712601	3.236518
-36.283052	20.490841	3.246515
-36.223706	25.775236	3.256512
-36.104693	26.947156	3.266509
-35.621699	21.915621	3.276506
-34.783433	16.516886	3.286502
-34.230747	14.602679	3.296499
-33.645535	22.324531	3.306496
-32.946563	16.662849	3.316493
-32.496718	14.321327	3.326490
-32.422911	20.111749	3.336486
-32.439394	16.695523	3.346483
-31.352370	28.577527	3.356480
-30.874270	22.175639	3.366477
-29.701588	26.123337	3.376474
-29.637149	16.011244	3.386470
-29.619515	18.538925	3.396467
-29.215130	14.324152	3.406464
-28.136072	15.252860	3.416461
-28.079515	16.282635	3.426458
-27.318535	18.047626	3.436454
-26.339876	20.456544	3.446451
-26.325099	18.026503	3.456448
-26.009234	20.183074	3.466445
-24.939223	11.954334	3.476442
-24.622328	20.077319	3.486438
-24.585089	23.322111	3.496435
-24.169152	16.352293	3.506432
-23.063437	23.529347	3.516429
-23.017046	14.188596	3.526426
-21.851681	21.939974	3.536422
-21.489973	19.172066	3.546419
-21.466447	24.301321	3.556416
-21.211273	17.879774	3.566413
-20.452917	23.187191	3.576410
-19.928342	23.426532	3.586406
-18.594833	22.377753	3.596403
-19.070921	25.572888	3.606400
-18.181989	25.667066	3.616397
-17.975226	17.829561	3.626394
-17.344362	14.266547	3.636390
-16.559231	18.579766	3.646387
-16.288596	16.762698	3.656384
-16.116079	18.865664	3.666381
-15.185594	13.985249	3.676378
-14.821170	12.566914	3.686374
-13.934930	22.857966	3.696371
-13.553529	21.500439	3.706368
-13.564612	21.268172	3.716365
-13.014206	22.269972	3.726362
-12.235436	23.442509	3.736358
-11.991704	23.168231	3.746355
-11.131942	20.759709	3.756352
-10.705556	14.980879	3.766349
-10.532185	22.363180	3.776346
-9.240655	26.104943	3.786342
-9.205547	24.896508	3.796339
-9.056255	24.573086	3.806336
-8.588488	12.464829	3.816333
-7.614134	21.078168	3.826330
-7.292106	15.709183	3.836326
-6.698380	19.158993	3.846323
-5.714387	20.548912	3.856320
-5.550281	19.241074	3.866317
-5.600442	19.450784	3.876314
-5.094794	26.659641	3.886310
-4.310200	26.907973	3.896307
-3.863890	28.275126	3.906304
-2.761777	31.663201	3.916301
-2.794081	36.520165	3.926298
-2.794008	37.638152	3.936294
-2.000360	54.448635	3.946291
-1.918862	55.811378	3.956288
-1.353279	68.783444	3.966285
-0.815221	92.879399	3.976282
-0.129994	110.167683	3.986278
0.000000	122.596804	3.991283
0.341631	120.464303	3.996288
0.476034	137.255336	4.001293
0.515876	146.991863	4.006298
0.938979	138.163755	4.011302
0.937361	136.514555	4.016307
0.968545	145.615897	4.021312
0.668960	150.200863	4.026317
0.375052	151.783041	4.031322
1.095831	156.671251	4.036326
1.167589	163.948886	4.041331
1.161494	173.400709	4.046336
1.262046	155.281951	4.051341
0.949533	163.941503	4.056346
0.856647	166.558988	4.061350
1.155903	173.140909	4.066355
1.180606	169.991855	4.071360
1.227818	162.004925	4.076365
1.034180	165.669305	4.081370
1.319002	153.180093	4.086374
1.061959	157.276203	4.091379
1.134619	175.662460	4.096384
1.391314	163.888494	4.101389
1.426923	168.525013	4.106394
0.858216	157.069176	4.111398
1.039295	159.752568	4.116403
1.106380	173.471426	4.121408
1.264588	175.625572	4.126413
0.866466	189.414415	4.131418
1.188650	164.934385	4.136422
1.290702	183.725900	4.141427
1.561880	175.917215	4.146432
1.270967	170.560147	4.151437
1.007304	177.970761	4.156442
1.205623	179.320263	4.161446
1.308906	186.490986	4.166451
1.187753	173.245872	4.171456
1.441469	171.423855	4.176461
1.127285	186.453510	4.181466
1.045235	185.927164	4.186470
1.203388	184.484380	4.191475
1.236905	187.651991	4.196480
1.526196	188.384176	4.201485
1.488360	177.959237	4.206490
1.466019	191.715184	4.211494
1.316688	184.219958	4.216499
1.837750	196.493702	4.221504
1.583704	185.332516	4.226509
1.528289	182.511407	4.231514
1.520217	173.687843	4.236518
1.331061	181.756205	4.241523
1.363538	179.302266	4.246528
1.868903	187.691912	4.251533
1.497528	188.140137	4.256538
1.515650	182.968865	4.261542
1.858939	182.327242	4.266547
1.827658	190.598004	4.271552
1.828656	181.786057	4.276557
1.670016	180.878440	4.281562
1.841235	184.588979	4.286566
1.592022	177.460781	4.291571
1.620352	173.615318	4.296576
1.965055	173.070835	4.301581
1.574856	187.805843	4.306586
1.715641	179.735763	4.311590
2.107661	179.786534	4.316595
1.804001	188.143938	4.321600
1.672363	180.229173	4.326605
1.757295	175.701730	4.331610
2.005862	178.324844	4.336614
1.737986	185.240912	4.341619
1.702349	190.194646	4.346624
1.740560	180.493790	4.351629
1.582480	187.693104	4.356634
1.692968	181.867682	4.361638
1.630283	187.664053	4.366643
1.488532	185.316151	4.371648
1.878545	193.842755	4.376653
1.827253	199.809103	4.381658
1.990689	213.232487	4.386662
2.141641	199.514124	4.391667
1.797319	197.193974	4.396672
2.140158	204.752785	4.401677
1.785132	197.701059	4.406682
1.691143	203.268304	4.411686
1.669476	211.366224	4.416691
1.899989	206.799028	4.421696
2.070498	209.667181	4.426701
2.001167	222.013551	4.431706
2.219129	204.159656	4.436710
2.003679	213.042235	4.441715
2.016611	207.578315	4.446720
2.323474	205.675297	4.451725
2.029783	212.042092	4.456730
1.958551	205.039555	4.461734
1.926375	218.023404	4.466739
1.972889	215.093696	4.471744
2.368513	208.884337	4.476749
1.894521	215.441046	4.481754
2.222201	201.508203	4.486758
2.124199	205.958258	4.491763
2.322410	223.948148	4.496768
2.543844	207.709737	4.501773
2.181568	213.560559	4.506778
2.259444	211.729712	4.511782
2.299074	210.272872	4.516787
2.649121	213.948243	4.521792
2.536901	207.956584	4.526797
2.319455	216.504760	4.531802
2.041054	197.786702	4.536806
1.730659	209.312040	4.541811
1.813195	215.612027	4.546816
2.411950	204.847170	4.551821
1.847912	218.938310	4.556826
2.286712	209.679801	4.561830
2.054010	205.840965	4.566835
1.984575	218.984971	4.571840
1.923330	216.361932	4.576845
2.285356	242.345690	4.581850
2.143247	249.336304	4.586854
2.229949	254.442783	4.591859
2.244825	249.391792	4.596864
2.525942	248.435571	4.601869
2.551577	238.597949	4.606874
2.282958	244.558498	4.611878
2.414518	255.743975	4.616883
2.137500	245.005035	4.621888
2.567411	246.978542	4.626893
2.408416	258.442197	4.631898
2.627099	246.212548	4.636902
2.595848	252.838664	4.641907
2.741912	251.163271	4.646912
2.731333	243.739499	4.651917
2.753931	256.574930	4.656922
2.561810	251.221240	4.661926
2.458685	246.001615	4.666931
2.382747	247.408087	4.671936
3.015475	243.065346	4.676941
2.837529	258.933518	4.681946
2.966630	252.095262	4.686950
2.846716	252.483583	4.691955
2.673944	240.201723	4.696960
2.907126	250.305424	4.701965
2.873923	256.848895	4.706970
3.093486	247.125723	4.711974
2.757159	238.927183	4.716979
2.429830	219.815166	4.721984
2.571237	233.672934	4.726989
2.650586	247.040494	4.731994
2.460369	238.483172	4.736998
2.465673	250.492559	4.742003
2.665791	252.478785	4.747008
2.652755	244.939696	4.752013
2.428649	248.865733	4.757018
2.622052	249.511560	4.762022
2.778958	242.124829	4.767027
2.627850	257.471910	4.772032
2.699511	247.146326	4.777037
2.942194	258.046086	4.782042
2.958100	271.105101	4.787046
2.707832	271.490203	4.792051
3.113895	283.691075	4.797056
3.199730	287.873015	4.802061
2.881294	268.398094	4.807066
2.934877	264.832660	4.812070
3.006635	270.352611	4.817075
2.988472	273.780054	4.822080
3.116459	278.864132	4.827085
2.870626	275.088614	4.832090
3.018350	267.381280	4.837094
3.211673	273.587117	4.842099
3.116491	276.642238	4.847104
3.369190	255.896095	4.852109
2.786125	260.588711	4.857114
2.998401	250.551243	4.862118
3.158000	262.913877	4.867123
2.691636	276.141482	4.872128
3.191736	271.882901	4.877133
3.121966	279.777487	4.882138
3.138396	286.924332	4.887142
3.459383	283.935738	4.892147
3.127987	283.137166	4.897152
3.522160	267.775404	4.902157
2.835202	273.313006	4.907162
3.220216	271.507854	4.912166
3.394690	277.165031	4.917171
2.980108	276.544368	4.922176
3.235241	274.340212	4.927181
3.243671	274.257063	4.932186
3.292762	281.975541	4.937190
3.145697	279.040914	4.942195
3.101903	277.003457	4.947200
3.382562	275.464555	4.952205
3.201906	275.127936	4.957210
3.275617	274.170966	4.962214
3.250806	277.114817	4.967219
3.399904	274.042952	4.972224
3.322274	273.375979	4.977229
3.102496	272.022773	4.982234
2.996616	269.538015	4.987238
3.220487	275.836375	4.992243
2.873546	275.562948	4.997248
3.668800	280.534883	5.002253
3.407773	309.053760	5.007258
3.343334	307.431004	5.012262
3.764938	308.560812	5.017267
3.293322	311.992463	5.022272
3.566851	306.862700	5.027277
3.380613	309.066880	5.032282
3.573672	310.714019	5.037286
3.464279	310.514000	5.042291
3.408948	311.883431	5.047296
3.633932	305.460823	5.052301
3.743704	310.318943	5.057306
3.316215	305.743451	5.062310
3.422525	305.771195	5.067315
3.431149	319.627701	5.072320
3.457680	317.867776	5.077325
3.655997	315.069134	5.082330
3.703359	311.813015	5.087334
3.652388	314.892309	5.092339
3.354663	308.815543	5.097344
3.740906	316.344053	5.102349
3.637591	321.968425	5.107354
3.714982	307.917716	5.112358
3.735162	307.944698	5.117363
3.240904	310.977479	5.122368
3.529260	306.412731	5.127373
3.404517	319.394303	5.132378
4.012755	331.532897	5.137382
4.133312	333.483744	5.142387
3.494706	322.689471	5.147392
3.839613	321.681664	5.152397
3.727328	340.896507	5.157402
4.053251	334.427807	5.162406
3.931893	333.323714	5.167411
3.825630	328.541031	5.172416
4.081540	331.717499	5.177421
3.699274	329.788553	5.182426
4.121412	320.835011	5.187430
3.937683	320.515077	5.192435
3.722239	324.748492	5.197440
4.103388	319.206517	5.202445
3.810557	330.182789	5.207450
3.772079	331.604388	5.212454
4.091400	329.222494	5.217459
3.737870	343.247489	5.222464
4.144376	345.344841	5.227469
3.706533	341.423458	5.232474
4.146355	345.178339	5.237478
4.469408	346.737999	5.242483
3.859396	353.710386	5.247488
4.177672	348.434111	5.252493
3.781604	350.625322	5.257498
4.014324	349.596590	5.262502
4.511246	347.599796	5.267507
4.229028	347.133948	5.272512
4.113543	342.248408	5.277517
4.128312	345.355911	5.282522
4.120024	340.857045	5.287526
4.377443	344.147411	5.292531
4.226999	343.931977	5.297536
4.335109	342.192703	5.302541
4.434602	344.551815	5.307546
3.870198	339.196475	5.312550
4.316759	330.343170	5.317555
4.201147	344.041466	5.322560
4.116218	334.920534	5.327565
4.118566	362.286014	5.332570
4.165091	347.824043	5.337574
4.410821	343.395369	5.342579
4.334323	346.928856	5.347584
4.436054	344.618927	5.352589
4.222459	347.489019	5.357594
4.361861	352.713299	5.362598
4.146986	346.806523	5.367603
4.111898	355.568123	5.372608
3.963128	348.337811	5.377613
3.862283	349.259176	5.382618
4.026293	350.303106	5.387622
4.374518	353.383919	5.392627
4.375616	354.336582	5.397632
4.598725	358.913564	5.402637
4.574292	363.684667	5.407642
4.003751	358.830517	5.412646
4.303830	367.690935	5.417651
4.458642	382.191533	5.422656
4.972062	376.631626	5.427661
4.685315	376.467820	5.432666
4.663495	368.483409	5.437670
4.305902	360.356588	5.442675
4.484412	369.335850	5.447680
4.898061	370.209092	5.452685
4.506829	359.153714	5.457690
4.283897	350.581610	5.462694
4.477886	367.454501	5.467699
4.534884	377.907046	5.472704
4.871384	374.927512	5.477709
4.984294	392.302963	5.482714
4.489414	377.881401	5.487718
4.704467	366.358040	5.492723
4.243758	385.724634	5.497728
4.742669	371.920992	5.502733
4.241578	376.346353	5.507738
4.052237	377.172541	5.512742
4.419176	378.128578	5.517747
4.469512	389.719435	5.522752
4.601912	378.523251	5.527757
4.627412	390.481463	5.532762
4.664024	396.157519	5.537766
4.934927	401.088288	5.542771
4.923618	414.761024	5.547776
5.103280	402.964385	5.552781
5.211471	386.549063	5.557786
4.564707	383.313617	5.562790
4.996262	374.488319	5.567795
4.656733	382.969649	5.572800
5.092342	381.917055	5.577805
4.847743	383.462399	5.582810
4.816312	389.561092	5.587814
4.935414	382.042423	5.592819
4.743564	377.872906	5.597824
5.090840	391.831066	5.602829
4.937431	392.109697	5.607834
4.747832	395.244077	5.612838
4.700374	396.199439	5.617843
4.797697	406.005556	5.622848
4.818034	399.077476	5.627853
5.207725	405.225562	5.632858
5.054018	410.592515	5.637862
4.983630	406.147103	5.642867
5.048841	407.994637	5.647872
4.922741	419.991736	5.652877
4.851079	410.120262	5.657882
4.904220	412.661764	5.662886
4.753482	412.412835	5.667891
4.899432	416.031318	5.672896
4.946235	406.266253	5.677901
4.944534	409.220714	5.682906
4.919157	420.858143	5.687910
5.037607	424.882998	5.692915
5.106187	454.891050	5.697920
5.138702	446.623553	5.702925
5.428861	448.607751	5.707930
5.261562	446.102037	5.712934
5.551507	435.135888	5.717939
5.095601	443.703865	5.722944
5.115531	446.348333	5.727949
5.538022	439.903686	5.732954
5.107685	447.793225	5.737958
5.441673	440.944999	5.742963
5.285507	448.919062	5.747968
5.215496	449.498526	5.752973
5.206900	449.146195	5.757978
5.276520	448.469876	5.762982
5.382928	442.433611	5.767987
5.244390	450.565472	5.772992
5.173283	449.609140	5.777997
5.609326	448.539600	5.783002
5.317058	450.982410	5.788006
5.741308	445.232009	5.793011
5.372606	449.934244	5.798016
5.410382	451.608342	5.803021
5.204323	458.252483	5.808026
5.120772	460.796456	5.813030
5.262874	453.293584	5.818035
5.255529	456.642131	5.823040
5.408073	446.912841	5.828045
5.158106	447.316444	5.833050
5.284702	457.069217	5.838054
5.478226	449.861217	5.843059
5.343731	468.499199	5.848064
5.389073	476.622589	5.853069
5.359493	478.794788	5.858074
5.574023	479.581173	5.863078
5.732904	477.682450	5.868083
5.439916	483.135684	5.873088
5.366023	485.759160	5.878093
5.433152	478.782566	5.883098
5.600102	484.650313	5.888102
5.917482	489.052327	5.893107
5.775062	492.350297	5.898112
5.863457	481.300415	5.903117
5.261014	494.869651	5.908122
5.257502	477.696560	5.913126
5.405638	480.883964	5.918131
5.282343	495.667305	5.923136
5.815104	489.752845	5.928141
6.205300	505.055214	5.933146
5.792301	503.304663	5.938150
5.982102	487.984249	5.943155
5.809208	487.557058	5.948160
5.950987	491.099197	5.953165
6.158565	480.989843	5.958170
5.872150	492.795066	5.963174
5.984964	483.769227	5.968179
5.791973	481.327046	5.973184
6.108078	487.181787	5.978189
5.982037	481.976524	5.983194
5.870035	483.486943	5.988198
5.872966	481.181877	5.993203
5.678370	479.252481	5.998208
6.175029	478.142240	6.003213
5.770007	482.217113	6.008218
5.852018	479.240645	6.013222
6.008467	475.110029	6.018227
5.674427	477.990677	6.023232
6.120159	477.276867	6.028237
6.046595	475.883103	6.033242
5.775382	477.929983	6.038246
6.138691	476.714710	6.043251
5.677676	480.386650	6.048256
6.010489	479.798147	6.053261
5.938732	486.542046	6.058266
5.829004	481.408967	6.063270
6.306262	486.025972	6.068275
5.821693	483.163555	6.073280
6.056894	483.816692	6.078285
5.945210	483.565451	6.083290
6.028245	486.554463	6.088294
5.994126	483.289970	6.093299
5.907321	479.569611	6.098304
5.922370	470.418561	6.103309
5.632035	476.008881	6.108314
5.437682	484.108055	6.113318
5.880685	473.773142	6.118323
5.509811	475.689494	6.123328
5.772844	482.149577	6.128333
5.827757	490.644610	6.133338
6.015038	496.093263	6.138342
5.987224	505.986421	6.143347
6.044815	506.424537	6.148352
5.973007	484.619164	6.153357
6.113734	492.155184	6.158362
5.984230	488.197705	6.163366
6.111046	477.468326	6.168371
5.776467	486.123516	6.173376
6.301554	488.640709	6.178381
6.294464	478.808637	6.183386
5.925851	482.095840	6.188390
6.291607	482.930733	6.193395
5.950531	489.914380	6.198400
5.854866	489.541414	6.203405
6.157077	479.184185	6.208410
5.896603	484.950312	6.213414
6.147372	486.005170	6.218419
6.112348	480.593670	6.223424
5.898648	487.298478	6.228429
6.165011	485.037485	6.233434
5.994644	478.862850	6.238438
6.045094	480.044929	6.243443
6.040242	476.098523	6.248448
6.394452	455.244573	6.253453
6.430873	454.174084	6.258458
5.687330	445.313362	6.263462
6.071540	436.898764	6.268467
6.040086	449.748221	6.273472
5.555750	448.453122	6.278477
6.128415	438.054680	6.283482
6.004912	453.153615	6.288486
6.075154	437.141699	6.293491
6.034896	447.337776	6.298496
6.164580	449.694776	6.303501
5.894463	448.961047	6.308506
6.071379	453.163497	6.313510
5.892792	446.648785	6.318515
5.775496	449.943087	6.323520
5.941347	458.914924	6.328525
6.070722	452.145395	6.333530
5.326258	454.436813	6.338534
6.108680	459.037022	6.343539
5.574827	450.404268	6.348544
5.590268	453.933141	6.353549
5.967047	455.018771	6.358554
5.515367	457.181795	6.363558
5.640946	448.645372	6.368563
5.801158	466.000364	6.373568
6.009758	478.971084	6.378573
5.897423	475.548152	6.383578
5.900438	486.869086	6.388582
6.284593	481.577242	6.393587
5.812481	466.879147	6.398592
6.048716	460.686754	6.403597
5.951854	454.772175	6.408602
5.653690	458.950237	6.413606
5.808236	469.857708	6.418611
5.780388	472.124922	6.423616
5.786387	488.840678	6.428621
5.727292	475.921268	6.433626
5.871870	482.899831	6.438630
5.973262	484.142157	6.443635
5.927209	483.288429	6.448640
6.045298	467.389133	6.453645
5.977503	485.723204	6.458650
5.917691	489.881913	6.463654
5.965728	481.606505	6.468659
5.583100	485.817079	6.473664
5.628014	480.514112	6.478669
5.848056	483.185204	6.483674
5.688004	501.043131	6.488678
5.852872	480.158875	6.493683
5.898914	490.099504	6.498688
5.840622	491.154530	6.503693
5.957790	486.087445	6.508698
5.665915	487.933917	6.513702
5.706838	486.919409	6.518707
5.882355	484.922931	6.523712
5.931854	484.348197	6.528717
6.361906	486.601206	6.533722
6.308830	484.711859	6.538726
6.427761	485.611021	6.543731
5.854737	480.192140	6.548736
5.831178	489.075921	6.553741
5.939458	484.999927	6.558746
5.643542	487.852276	6.563750
6.020315	477.750480	6.568755
5.787346	487.422896	6.573760
5.521956	483.845701	6.578765
5.692698	481.887994	6.583770
5.844522	488.602938	6.588774
6.075547	475.752295	6.593779
5.686901	487.961930	6.598784
5.727662	492.629858	6.603789
6.082650	484.509915	6.608794
5.488913	496.881901	6.613798
5.845457	484.645756	6.618803
5.804433	488.006091	6.623808
5.999296	505.956910	6.628813
5.872395	499.975455	6.633818
5.978250	508.689976	6.638822
5.985130	501.040921	6.643827
5.742269	498.673276	6.648832
6.227113	504.428119	6.653837
5.864314	489.789778	6.658842
5.722624	486.224993	6.663846
6.183575	499.396328	6.668851
5.910419	493.350945	6.673856
6.027338	484.503093	6.678861
5.783903	492.919473	6.683866
5.606731	499.135524	6.688870
6.164820	494.029411	6.693875
6.070310	506.460082	6.698880
5.890870	493.882461	6.703885
5.652186	482.945823	6.708890
6.017128	504.365900	6.713894
6.345845	500.066520	6.718899
5.698983	492.334603	6.723904
5.703946	495.746731	6.728909
6.066981	496.546263	6.733914
5.639828	483.296595	6.738918
6.127407	499.622703	6.743923
6.116200	496.667458	6.748928
5.884707	489.389287	6.753933
5.886330	490.665464	6.758938
5.764012	488.455186	6.763942
6.049860	488.015917	6.768947
5.848504	496.169135	6.773952
5.976037	490.270536	6.778957
6.008913	481.617511	6.783962
5.680746	490.313573	6.788966
6.205118	500.788805	6.793971
5.980353	493.552338	6.798976
6.119427	501.673866	6.803981
6.128052	492.340462	6.808986
6.026667	481.282776	6.813990
6.313661	485.985779	6.818995
5.833849	491.269518	6.824000
6.267686	486.827772	6.829005
6.652877	487.485128	6.834010
6.074191	486.645526	6.839014
6.005035	486.890207	6.844019
5.879726	488.092157	6.849024
6.079706	488.373458	6.854029
5.953871	475.819451	6.859034
6.018298	489.570008	6.864038
5.870127	492.306192	6.869043
6.010630	483.868307	6.874048
5.968446	471.074360	6.879053
6.044817	463.048517	6.884058
5.655155	468.642225	6.889062
6.046958	473.831643	6.894067
5.885177	483.914838	6.899072
5.956210	481.258646	6.904077
5.985536	471.106638	6.909082
5.894705	464.528975	6.914086
5.845870	453.177016	6.919091
5.620898	470.723524	6.924096
5.799663	477.880332	6.929101
5.964087	480.697450	6.934106
5.897081	498.795322	6.939110
6.086571	483.784942	6.944115
6.125081	494.261437	6.949120
5.899682	481.908366	6.954125
5.826371	485.250260	6.959130
5.746125	489.023245	6.964134
5.864575	484.092588	6.969139
5.623390	489.900417	6.974144
5.798966	487.336161	6.979149
5.955428	489.743003	6.984154
6.020631	488.243829	6.989158
6.084470	486.571936	6.994163
6.035691	494.165418	6.999168
6.026254	484.210608	7.004173
6.152572	474.076211	7.009178
5.817093	492.091865	7.014182
6.183924	486.658547	7.019187
6.073342	482.179307	7.024192
5.655277	483.788547	7.029197
6.215635	467.888577	7.034202
5.633925	470.833632	7.039206
6.089338	474.642007	7.044211
5.512379	476.307002	7.049216
5.754781	489.557262	7.054221
5.745411	487.817654	7.059226
5.954423	482.730558	7.064230
6.156508	490.859229	7.069235
5.894079	494.149308	7.074240
6.277765	495.804921	7.079245
5.976398	487.564264	7.084250
6.138508	494.687920	7.089254
6.085493	474.953705	7.094259
5.587798	466.551742	7.099264
5.389250	478.448390	7.104269
6.254930	478.125414	7.109274
5.728122	486.806353	7.114278
6.206726	490.821530	7.119283
6.365554	480.687084	7.124288
6.030574	473.317007	7.129293
5.809498	468.806899	7.134298
5.652778	458.907817	7.139302
5.798366	466.755071	7.144307
6.290484	481.000736	7.149312
6.125594	476.282943	7.154317
5.989509	454.790023	7.159322
5.604351	465.395015	7.164326
6.086006	453.910500	7.169331
5.699044	468.047484	7.174336
5.782176	457.934638	7.179341
5.861114	458.014655	7.184346
5.699732	479.648054	7.189350
5.509608	479.900295	7.194355
5.758857	494.931950	7.199360
5.910950	493.082689	7.204365
5.879351	487.440455	7.209370
5.922287	496.329333	7.214374
6.190596	490.318286	7.219379
6.040150	490.904729	7.224384
6.240462	495.641693	7.229389
6.158178	488.749176	7.234394
6.012551	488.270124	7.239398
5.985712	469.498225	7.244403
6.033845	466.194197	7.249408
6.062118	451.080955	7.254413
5.963535	460.887320	7.259418
5.562482	462.949735	7.264422
5.646484	457.275486	7.269427
6.029285	476.904233	7.274432
5.742923	485.111744	7.279437
5.928536	476.613923	7.284442
5.834597	486.581333	7.289446
6.135509	478.192020	7.294451
5.816060	485.833483	7.299456
5.703710	493.469139	7.304461
5.778339	480.887130	7.309466
5.435723	496.603008	7.314470
5.858285	486.532707	7.319475
5.939598	490.690490	7.324480
5.792052	491.361595	7.329485
6.155850	481.408840	7.334490
5.949218	494.996228	7.339494
6.108439	488.584313	7.344499
5.743802	487.446616	7.349504
6.123341	478.592168	7.354509
6.022150	484.193952	7.359514
5.948574	496.413385	7.364518
6.371401	486.584354	7.369523
6.011473	495.262779	7.374528
5.712764	486.034725	7.379533
5.976657	485.914982	7.384538
6.105695	483.333951	7.389542
6.096875	478.521504	7.394547
5.972629	473.634705	7.399552
5.782079	455.340046	7.404557
5.869864	471.282320	7.409562
5.859779	480.382294	7.414566
6.200561	478.273563	7.419571
5.876860	466.129424	7.424576
5.906271	482.076324	7.429581
5.913341	473.180631	7.434586
6.063535	463.333134	7.439590
5.820498	459.792600	7.444595
5.629309	462.777300	7.449600
6.041643	476.040507	7.454605
6.193297	470.539560	7.459610
5.920652	466.759645	7.464614
6.123966	452.393308	7.469619
6.315609	455.711340	7.474624
6.030977	450.742334	7.479629
6.269196	436.746715	7.484634
6.229004	459.796885	7.489638
6.096327	453.611494	7.494643
6.173277	453.024826	7.499648
6.090946	467.954288	7.504653
6.368931	451.121243	7.509658
6.087813	465.776338	7.514662
6.052832	451.984690	7.519667
5.666454	440.286989	7.524672
5.717180	458.643963	7.529677
5.871966	454.474165	7.534682
5.479796	457.629899	7.539686
5.796719	455.207440	7.544691
5.851698	454.004941	7.549696
5.880599	457.931149	7.554701
5.825773	444.619493	7.559706
5.867852	459.125771	7.564710
5.981344	450.191787	7.569715
5.793975	452.025622	7.574720
5.944497	464.871657	7.579725
6.138315	455.299113	7.584730
6.046337	460.374416	7.589734
5.868019	458.251828	7.594739
6.269308	460.582986	7.599744
6.015852	463.073547	7.604749
5.910055	454.223055	7.609754
5.839273	457.091765	7.614758
5.681486	464.482651	7.619763
6.026660	465.154215	7.624768
5.851741	464.597824	7.629773
6.193078	461.648255	7.634778
5.445399	461.615767	7.639782
5.795053	450.381853	7.644787
5.653588	463.909610	7.649792
5.719173	459.751986	7.654797
5.767380	448.179775	7.659802
5.704229	459.957352	7.664806
5.899754	458.512412	7.669811
6.123547	454.218841	7.674816
5.809661	456.311839	7.679821
5.999011	456.066592	7.684826
6.090007	456.748985	7.689830
5.916155	443.219140	7.694835
5.938327	452.862690	7.699840
5.728781	463.190539	7.704845
5.800037	454.278922	7.709850
5.851793	458.599825	7.714854
5.952615	453.990158	7.719859
5.921564	449.915889	7.724864
6.035059	453.291624	7.729869
6.086912	462.744308	7.734874
6.143254	461.717191	7.739878
6.269377	458.275279	7.744883
6.234414	468.123915	7.749888
5.786178	458.832586	7.754893
5.958571	450.374947	7.759898
5.910370	456.611793	7.764902
6.213258	454.504986	7.769907
6.392519	454.992350	7.774912
6.128131	465.889236	7.779917
5.972180	457.063901	7.784922
5.901285	463.781504	7.789926
5.738257	461.042451	7.794931
5.692748	446.727795	7.799936
5.775674	465.554287	7.804941
5.799491	447.756166	7.809946
6.078372	456.433777	7.814950
5.935388	465.385128	7.819955
5.996411	460.464561	7.824960
5.867777	460.467300	7.829965
5.953833	456.638667	7.834970
5.753102	455.210179	7.839974
5.976353	449.819248	7.844979
5.855158	449.425245	7.849984
5.556972	459.876361	7.854989
6.006065	452.628888	7.859994
5.828032	453.590441	7.864998
6.118082	447.425663	7.870003
5.853074	461.341130	7.875008
5.889264	456.941132	7.880013
6.016712	454.530353	7.885018
5.949494	456.476828	7.890022
5.858813	453.030493	7.895027
6.232169	456.104214	7.900032
5.649927	463.054303	7.905037
6.149378	451.794843	7.910042
6.038021	456.327484	7.915046
6.145257	452.394722	7.920051
6.068761	452.885481	7.925056
5.840417	463.225611	7.930061
6.248452	447.980458	7.935066
5.974811	462.980597	7.940070
6.386055	452.149774	7.945075
6.081428	432.374717	7.950080
5.901280	427.905903	7.955085
5.810496	422.058306	7.960090
5.757833	425.300289	7.965094
5.803805	421.592926	7.970099
5.701345	424.000913	7.975104
5.647577	431.795658	7.980109
5.901482	449.688904	7.985114
5.838859	457.627092	7.990118
6.029464	455.199723	7.995136
6.224387	464.450037	8.000154
5.768757	452.489608	8.005171
6.128654	459.354492	8.010189
6.059666	457.543767	8.015206
5.832635	441.075154	8.020224
6.039459	448.246077	8.025242
5.550152	439.137375	8.030259
6.071528	454.815140	8.035277
5.783563	456.972451	8.040294
6.225854	462.945756	8.045312
6.368511	454.238410	8.050330
5.629583	453.254484	8.055347
6.075453	449.498637	8.060365
5.871375	466.686950	8.065382
6.193304	468.388038	8.070400
6.110627	453.977796	8.075418
5.908891	438.265868	8.080435
5.964392	440.855980	8.085453
5.699375	464.873589	8.090470
5.965698	461.016138	8.095488
6.318277	461.261776	8.100506
6.160578	468.000531	8.105523
5.987508	461.018430	8.110541
6.388999	467.873886	8.115558
5.932551	446.783134	8.120576
5.928962	442.075205	8.125594
5.706931	464.929558	8.130611
6.139340	457.480745	8.135629
6.087980	462.620663	8.140646
5.903249	465.011945	8.145664
5.942921	457.606188	8.150682
6.263425	476.461686	8.155699
6.280354	463.795334	8.160717
5.926343	461.216724	8.165734
5.854654	471.155355	8.170752
6.033663	457.139175	8.175770
5.737763	464.140775	8.180787
6.172022	462.981279	8.185805
5.960043	451.144922	8.190822
5.997821	467.984771	8.195840
6.144074	462.443090	8.200858
6.383393	463.449218	8.205875
5.918026	473.261413	8.210893
6.183906	463.056153	8.215910
6.163238	456.945137	8.220928
6.385290	467.524744	8.225946
5.879434	465.621975	8.230963
6.084709	464.770932	8.235981
5.973672	467.008629	8.240998
6.006505	463.585644	8.246016
5.946189	454.856831	8.251034
5.886586	455.894152	8.256051
5.919216	466.177767	8.261069
6.069668	482.190422	8.266086
6.406155	489.431158	8.271104
6.348420	487.480016	8.276122
6.432786	498.019713	8.281139
6.017194	490.319468	8.286157
6.208677	488.989110	8.291174
6.234113	491.349995	8.296192
6.348395	483.201930	8.301210
5.903276	494.877528	8.306227
6.050547	499.437701	8.311245
6.316765	494.942104	8.316262
6.191833	491.593895	8.321280
6.106654	490.227088	8.326298
6.001956	495.144384	8.331315
6.202102	488.982694	8.336333
6.155111	491.171334	8.341350
6.136428	490.030006	8.346368
6.198079	493.351437	8.351386
6.221018	493.911437	8.356403
6.454752	492.851991	8.361421
6.296033	488.532503	8.366438
6.198802	503.032792	8.371456
6.097128	494.276152	8.376474
6.307476	497.063177	8.381491
6.433092	484.824719	8.386509
6.211504	487.545158	8.391526
6.290401	499.832148	8.396544
6.415307	485.158880	8.401562
6.072694	495.617986	8.406579
6.299894	497.599146	8.411597
6.389827	493.322504	8.416614
6.078861	494.437776	8.421632
6.429626	490.414426	8.426650
6.277777	491.158593	8.431667
6.824679	497.037968	8.436685
6.275603	496.810395	8.441702
6.206764	500.994556	8.446720
6.489219	484.341329	8.451738
6.223233	499.775907	8.456755
6.425047	500.020187	8.461773
6.202327	502.383901	8.466790
6.297718	519.030465	8.471808
6.531248	522.427611	8.476826
6.562986	530.553792	8.481843
6.612828	527.042173	8.486861
6.371304	518.971978	8.491878
6.298980	526.521677	8.496896
6.625637	515.795913	8.501914
6.487238	528.226194	8.506931
6.576874	511.478647	8.511949
6.619257	506.825883	8.516966
6.149089	516.733170	8.521984
6.166188	509.072511	8.527002
6.432257	521.393633	8.532019
6.075514	536.831143	8.537037
6.487806	531.949463	8.542054
6.405842	534.803792	8.547072
6.908862	536.661931	8.552090
6.537681	531.861406	8.557107
6.477319	539.473294	8.562125
6.712147	538.829328	8.567143
6.305049	530.701761	8.572160
6.677328	535.398741	8.577178
6.638415	531.728005	8.582195
6.499430	531.487377	8.587213
6.574153	521.382847	8.592231
6.754142	526.939973	8.597248
6.865138	528.079887	8.602266
6.728219	530.769022	8.607283
6.803614	526.346477	8.612301
6.382809	505.807217	8.617319
6.232071	513.961478	8.622336
6.414765	528.659773	8.627354
6.294466	534.084181	8.632371
6.650252	543.829605	8.637389
6.582953	526.378400	8.642407
6.580707	528.568409	8.647424
6.727684	539.317723	8.652442
6.545363	532.314092	8.657459
6.436897	536.239806	8.662477
6.707803	536.446788	8.667495
6.302069	533.910269	8.672512
6.616177	530.073441	8.677530
6.396864	537.005934	8.682547
6.374431	533.090102	8.687565
6.217444	536.357043	8.692583
6.256115	543.070760	8.697600
6.636005	549.634214	8.702618
6.697308	561.459788	8.707635
6.899352	553.700841	8.712653
7.066274	563.422872	8.717671
6.521845	557.270148	8.722688
6.710693	546.851822	8.727706
6.955946	540.623517	8.732723
6.869515	552.159978	8.737741
6.813457	523.259952	8.742759
6.732951	537.942413	8.747776
7.060024	529.938748	8.752794
6.721502	529.252944	8.757811
6.530852	536.144978	8.762829
7.073031	530.676498	8.767847
6.696104	538.569195	8.772864
6.389696	533.733364	8.777882
6.764937	532.826578	8.782899
6.503342	542.245668	8.787917
6.728859	536.567266	8.792935
6.622580	557.279244	8.797952
6.816544	563.516710	8.802970
6.874655	564.386388	8.807987
6.802832	575.323822	8.813005
6.977625	560.200202	8.818023
7.035137	568.357176	8.823040
6.899728	548.819400	8.828058
6.673428	538.419990	8.833075
6.279384	545.448571	8.838093
6.623447	552.377913	8.843111
6.717603	564.675816	8.848128
6.898950	562.750988	8.853146
7.068588	562.775435	8.858163
6.892598	581.751783	8.863181
6.755666	572.018251	8.868199
6.671736	572.587451	8.873216
6.737294	578.125325	8.878234
6.999877	567.174040	8.883251
6.714825	570.020410	8.888269
6.831909	565.124623	8.893287
6.612707	564.230161	8.898304
6.882131	570.511743	8.903322
6.964004	566.005555	8.908339
6.834999	574.889473	8.913357
7.247719	577.815278	8.918375
6.767021	564.910081	8.923392
6.736174	562.737404	8.928410
7.198358	555.961241	8.933427
6.807582	567.767944	8.938445
6.839767	566.602557	8.943463
6.763000	566.847018	8.948480
6.885472	561.605234	8.953498
7.024922	572.912395	8.958515
6.841173	573.973585	8.963533
7.003903	564.205102	8.968551
6.859113	570.047364	8.973568
7.048745	582.369751	8.978586
6.908494	573.039343	8.983603
6.813813	588.621355	8.988621
7.191044	591.239214	8.993639
7.223805	605.154550	8.998656
6.959851	595.813671	9.003674
7.403501	588.087502	9.008691
7.358288	587.581525	9.013709
7.178978	575.535679	9.018727
7.171896	571.173395	9.023744
7.024159	573.025027	9.028762
7.091161	571.111025	9.033779
6.985223	581.097012	9.038797
7.200344	581.599868	9.043815
7.191494	572.259653	9.048832
7.036638	569.582870	9.053850
6.876345	567.328947	9.058867
7.206851	571.510802	9.063885
7.206017	568.370565	9.068903
7.254092	574.714707	9.073920
7.492987	573.333503	9.078938
7.292345	568.245782	9.083955
6.546558	576.371663	9.088973
7.469929	574.479692	9.093991
7.340807	564.397209	9.099008
7.251688	576.177095	9.104026
6.858081	577.916240	9.109043
6.862687	570.201819	9.114061
7.172710	571.122466	9.119079
7.019398	570.414024	9.124096
6.880697	572.453298	9.129114
7.237546	563.042716	9.134131
6.935032	571.608329	9.139149
7.266430	595.814138	9.144167
7.454528	593.234385	9.149184
7.049356	594.629155	9.154202
7.360478	584.152318	9.159219
7.029821	588.458690	9.164237
6.980440	596.660995	9.169255
7.309730	604.280851	9.174272
7.263602	604.683012	9.179290
7.466863	600.184405	9.184307
7.153643	602.795917	9.189325
7.421607	606.824666	9.194343
7.435197	605.597598	9.199360
7.429228	594.285144	9.204378
7.608788	584.222783	9.209395
7.109000	573.440678	9.214413
7.330672	569.601010	9.219431
7.098884	576.608598	9.224448
7.106203	588.711957	9.229466
7.621684	598.014475	9.234483
7.279038	603.895252	9.239501
7.416654	597.084439	9.244519
7.549483	603.428756	9.249536
7.245706	586.309516	9.254554
7.262606	563.956367	9.259571
7.277826	589.293822	9.264589
7.716826	592.920854	9.269607
7.663842	570.529451	9.274624
7.389432	576.391659	9.279642
7.290849	566.938447	9.284659
7.158191	570.829101	9.289677
7.373768	568.568073	9.294695
7.451350	573.116069	9.299712
7.028822	577.836161	9.304730
7.427287	591.034392	9.309747
7.370680	593.435026	9.314765
7.697374	596.853696	9.319783
7.637728	605.293874	9.324800
7.246883	597.902513	9.329818
7.388695	592.072011	9.334835
7.520224	596.557173	9.339853
7.208716	597.852328	9.344871
7.260509	598.562847	9.349888
7.173713	606.344753	9.354906
7.252042	606.251048	9.359923
7.334258	595.642084	9.364941
7.489045	607.161752	9.369959
7.283665	607.656948	9.374976
7.570616	591.211875	9.379994
7.639596	589.810531	9.385011
7.362706	603.578652	9.390029
7.295780	595.451715	9.395047
7.604370	603.329566	9.400064
7.216783	602.328310	9.405082
7.778324	592.890182	9.410099
7.234340	601.852926	9.415117
7.418346	598.612565	9.420135
7.436259	595.941373	9.425152
7.495156	616.836034	9.430170
7.768649	627.959699	9.435187
7.763480	635.535748	9.440205
7.684729	625.703707	9.445223
7.705943	605.907640	9.450240
7.619455	599.184735	9.455258
7.625343	594.792059	9.460275
7.388478	607.896517	9.465293
7.736367	613.180013	9.470311
7.617647	607.596849	9.475328
7.864675	619.576876	9.480346
7.628307	598.588297	9.485363
7.175529	615.003078	9.490381
7.878088	627.198818	9.495399
7.963550	618.849776	9.500416
7.492994	622.639522	9.505434
7.349327	618.643428	9.510451
7.551767	639.637308	9.515469
7.771484	628.550177	9.520487
8.020012	635.387885	9.525504
7.656626	647.009253	9.530522
7.671434	632.450378	9.535539
7.952277	629.568736	9.540557
7.681514	637.722132	9.545575
7.909849	632.083969	9.550592
7.823752	630.989393	9.555610
7.791896	633.853665	9.560627
7.978244	624.035482	9.565645
7.660331	620.995950	9.570663
7.658684	619.405527	9.575680
7.626148	633.828726	9.580698
7.838435	618.686454	9.585715
7.651032	646.022054	9.590733
7.987164	631.312954	9.595751
7.923657	625.503577	9.600768
7.729996	642.537737	9.605786
7.687864	636.088237	9.610803
8.032998	633.262689	9.615821
7.529833	641.155241	9.620839
7.832533	626.213136	9.625856
7.754863	640.904574	9.630874
7.643975	632.069769	9.635891
7.352900	631.915086	9.640909
7.497947	638.253267	9.645927
7.698054	635.662863	9.650944
7.326034	629.100002	9.655962
7.744603	637.521100	9.660979
7.865600	657.646060	9.665997
8.204769	661.786063	9.671015
8.076386	649.785669	9.676032
7.807422	652.182831	9.681050
7.745225	631.626357	9.686067
7.976101	648.299185	9.691085
7.591286	670.374111	9.696103
8.243525	660.388775	9.701120
7.986489	658.588732	9.706138
8.077594	660.036410	9.711155
7.720852	662.387756	9.716173
7.822484	675.322969	9.721191
8.229336	662.416462	9.726208
8.060869	676.055039	9.731226
8.046118	667.200194	9.736243
8.444260	666.535040	9.741261
8.096781	655.807415	9.746279
7.837706	643.220477	9.751296
7.813770	640.945092	9.756314
8.271144	648.001294	9.761331
8.016611	648.312132	9.766349
7.572561	639.059343	9.771367
8.282297	657.451510	9.776384
8.004815	663.341517	9.781402
8.161863	672.552162	9.786419
8.046909	670.195278	9.791437
8.189232	675.556951	9.796455
8.197157	662.333962	9.801472
7.914485	665.240771	9.806490
8.296917	666.522909	9.811507
8.405109	677.494927	9.816525
8.078724	650.280942	9.821543
8.196060	642.772417	9.826560
7.896534	653.507820	9.831578
8.133899	659.233332	9.836595
8.436581	664.099400	9.841613
7.905730	667.837519	9.846631
8.335149	664.766685	9.851648
7.618387	661.292170	9.856666
8.138086	676.490515	9.861683
8.196793	674.542740	9.866701
8.025695	680.681164	9.871719
8.237050	665.995013	9.876736
8.296397	676.796594	9.881754
8.048172	670.580507	9.886771
7.815135	673.737529	9.891789
8.373253	674.274634	9.896807
8.033657	680.317699	9.901824
7.954541	682.524566	9.906842
8.001211	683.181419	9.911859
8.113767	672.386125	9.916877
7.679092	685.778406	9.921895
8.309941	681.082074	9.926912
8.572087	691.216614	9.931930
8.127515	691.206171	9.936947
8.407711	686.434346	9.941965
8.245425	689.909043	9.946983
8.274085	681.164119	9.952000
8.083797	680.965128	9.957018
8.388241	696.242560	9.962035
8.571114	688.977758	9.967053
8.619508	695.159134	9.972071
8.189681	686.208237	9.977088
8.369124	686.372867	9.982106
8.327252	696.278276	9.987123
8.592417	685.725615	9.992141
8.256671	680.830031	9.997159
8.273725	688.712510	10.002176
8.177049	693.277825	10.007194
8.225246	696.406581	10.012211
8.607777	698.975954	10.017229
8.324967	696.666093	10.022247
8.517401	696.769828	10.027264
8.678000	696.613816	10.032282
8.408809	707.487325	10.037299
8.453966	703.896633	10.042317
8.656288	709.916383	10.047335
8.546742	694.739836	10.052352
8.453716	690.584301	10.057370
8.147648	696.554522	10.062387
8.628951	694.636004	10.067405
8.278738	705.277280	10.072423
8.702168	702.032266	10.077440
8.162819	706.998331	10.082458
8.463228	704.939856	10.087475
8.621775	705.818628	10.092493
8.216583	711.387993	10.097511
8.590015	712.588961	10.102528
8.513949	696.136260	10.107546
8.373245	706.632897	10.112563
8.471266	702.067810	10.117581
8.311786	703.844445	10.122599
8.525115	702.278024	10.127616
8.653129	699.488836	10.132634
8.279004	707.756871	10.137651
8.698128	696.359136	10.142669
8.439698	701.776120	10.147687
8.377415	703.524097	10.152704
8.666113	700.705698	10.157722
8.363019	707.593462	10.162739
8.730932	700.566430	10.167757
8.737478	699.803814	10.172775
8.439564	707.138076	10.177792
8.607223	706.973615	10.182810
8.771782	716.290209	10.187827
8.564808	708.350202	10.192845
8.533285	715.656191	10.197863
8.873084	729.053372	10.202880
8.744503	734.580184	10.207898
8.299788	727.928033	10.212915
8.614677	731.369054	10.217933
8.895501	739.844167	10.222951
9.248664	733.153450	10.227968
8.624751	734.477018	10.232986
8.253149	737.966931	10.238003
8.650527	726.654642	10.243021
8.895153	733.662789	10.248039
8.838461	740.657458	10.253056
8.871296	742.017252	10.258074
8.853377	743.706436	10.263091
9.089172	732.349795	10.268109
8.847859	739.588317	10.273127
9.119566	737.630134	10.278144
9.104689	701.369955	10.283162
8.648249	719.340168	10.288179
8.693707	709.389633	10.293197
8.662898	711.466794	10.298215
8.713181	727.546346	10.303232
8.996069	735.446521	10.308250
8.820899	739.458788	10.313267
8.845194	738.284752	10.318285
9.296332	730.864794	10.323303
8.632467	724.446755	10.328320
8.831328	720.875433	10.333338
8.785403	727.349126	10.338355
8.840648	724.585047	10.343373
8.904303	735.240907	10.348391
8.968082	730.713945	10.353408
9.142948	739.250358	10.358426
8.807514	742.175445	10.363443
8.788360	736.961238	10.368461
8.621526	731.374860	10.373479
8.788268	736.108230	10.378496
9.057500	745.078178	10.383514
8.656885	734.617891	10.388531
9.194243	735.347763	10.393549
8.994830	737.327124	10.398567
8.906891	732.642099	10.403584
9.129525	733.729531	10.408602
9.020051	737.905218	10.413619
8.937934	729.184182	10.418637
9.226735	739.132396	10.423655
8.836098	735.886790	10.428672
9.218287	729.723558	10.433690
8.907780	737.313409	10.438707
9.065030	743.827634	10.443725
9.042913	745.176336	10.448743
9.079040	739.953878	10.453760
9.144452	737.418092	10.458778
8.858837	739.836027	10.463795
9.102831	735.040942	10.468813
8.942950	730.722955	10.473831
8.982009	735.414543	10.478848
9.095917	738.683798	10.483866
8.732289	734.874486	10.488883
9.143089	751.564338	10.493901
9.389580	757.662618	10.498919
9.203116	760.599501	10.503936
9.224855	757.396157	10.508954
9.018368	766.743395	10.513971
9.001807	767.331582	10.518989
9.343235	767.892690	10.524007
8.948622	769.873414	10.529024
9.040319	765.000161	10.534042
8.816227	770.394274	10.539059
8.937654	769.289700	10.544077
9.162977	770.131264	10.549095
9.118000	772.298454	10.554112
9.298613	768.618151	10.559130
9.323992	768.194677	10.564147
9.357832	782.388781	10.569165
9.453324	773.041140	10.574183
9.241118	772.869190	10.579200
9.246286	770.364512	10.584218
9.103135	775.316002	10.589235
9.480559	762.493787	10.594253
9.358307	776.936669	10.599271
9.195160	776.292134	10.604288
9.176398	771.121936	10.609306
9.096909	771.979528	10.614323
9.474939	776.425975	10.619341
9.556546	775.674176	10.624359
9.313174	767.207577	10.629376
9.651048	771.877644	10.634394
9.387218	767.129370	10.639411
9.299974	766.017458	10.644429
9.127285	769.940559	10.649447
9.127940	776.666270	10.654464
9.512499	784.142857	10.659482
9.627794	811.632528	10.664499
9.505716	793.746357	10.669517
9.638314	790.712543	10.674535
9.053313	785.879470	10.679552
9.582978	790.609761	10.684570
9.345401	801.120601	10.689587
9.646793	802.521536	10.694605
9.823757	805.488118	10.699623
9.618794	789.235423	10.704640
9.492367	777.620458	10.709658
9.595359	772.065151	10.714675
9.234278	771.892808	10.719693
9.852652	776.536205	10.724711
9.377774	783.675183	10.729728
9.707694	791.145844	10.734746
9.398142	787.556083	10.739763
9.537500	795.654975	10.744781
9.837272	793.289959	10.749799
9.587908	801.399165	10.754816
9.994466	789.264208	10.759834
9.548739	782.065650	10.764851
9.480646	777.301165	10.769869
9.502803	778.250109	10.774887
9.292253	782.905809	10.779904
9.701509	792.364458	10.784922
9.928321	813.445081	10.789939
9.839263	809.338653	10.794957
9.712505	794.395025	10.799975
9.396716	795.948729	10.804992
9.837687	797.076054	10.810010
9.996415	800.395877	10.815027
9.746138	787.554461	10.820045
9.811581	772.209773	10.825063
9.263514	785.754121	10.830080
9.493092	786.849462	10.835098
9.901172	798.570284	10.840115
9.940063	808.781257	10.845133
10.015089	815.129605	10.850151
9.907020	802.180342	10.855168
9.830097	784.950176	10.860186
9.746639	785.760206	10.865203
9.598521	784.357326	10.870221
9.645252	790.984107	10.875239
9.780837	804.959291	10.880256
9.802514	805.199394	10.885274
10.188119	801.042279	10.890291
10.064880	806.929780	10.895309
9.717387	794.623715	10.900327
9.768738	807.170770	10.905344
9.947920	809.489174	10.910362
9.933970	803.728813	10.915379
9.747464	809.761095	10.920397
9.837802	808.223451	10.925415
9.545405	814.055755	10.930432
9.945044	809.850756	10.935450
9.910608	807.212288	10.940467
10.035493	799.274076	10.945485
9.964175	805.936609	10.950503
9.449560	799.264979	10.955520
10.101095	816.358442	10.960538
10.142093	817.473829	10.965555
9.754910	816.328620	10.970573
9.999386	813.038662	10.975591
9.846948	814.511840	10.980608
10.083707	806.164363	10.985626
10.130173	815.745073	10.990643
9.915483	806.093029	10.995661
10.146722	806.108674	11.000679
9.887257	804.637497	11.005696
9.904102	800.233406	11.010714
9.837680	815.429454	11.015731
9.851411	809.523401	11.020749
10.034539	808.734256	11.025767
9.787304	808.990752	11.030784
9.725323	816.502177	11.035802
9.973025	832.252420	11.040819
10.060982	839.109078	11.045837
10.408649	837.877759	11.050855
10.410656	840.641019	11.055872
10.275779	839.116086	11.060890
10.267513	828.890547	11.065907
10.023996	818.567597	11.070925
10.475820	819.047287	11.075943
10.100893	813.050862	11.080960
9.909221	807.448486	11.085978
10.077589	817.377094	11.090995
9.983781	839.291299	11.096013
10.366247	833.032821	11.101031
10.226472	834.781219	11.106048
10.159660	843.549423	11.111066
10.701157	833.227815	11.116083
10.397214	833.421255	11.121101
10.247754	823.521357	11.126119
10.274178	823.747391	11.131136
10.259273	836.343601	11.136154
10.260562	840.674208	11.141171
10.334643	841.435770	11.146189
10.177110	837.546713	11.151207
10.458042	835.971764	11.156224
10.481530	828.682655	11.161242
10.653773	832.740567	11.166259
10.360700	824.121451	11.171277
10.552092	800.442909	11.176295
9.850366	816.127238	11.181312
10.440955	813.579343	11.186330
10.342981	814.685517	11.191347
10.335061	835.043489	11.196365
10.623294	836.125599	11.201383
10.211911	841.335668	11.206400
10.257238	840.040849	11.211418
10.393932	831.918123	11.216435
10.400907	830.504862	11.221453
10.378759	825.679925	11.226471
10.482003	827.560374	11.231488
10.455668	840.563322	11.236506
10.725371	839.411606	11.241523
10.388821	846.575776	11.246541
10.516714	828.497103	11.251559
10.328766	837.669797	11.256576
10.558143	848.006375	11.261594
10.643458	842.115837	11.266611
10.397919	850.650244	11.271629
10.579990	843.166842	11.276647
10.161168	840.187930	11.281664
10.318483	847.562264	11.286682
10.568518	829.628138	11.291699
10.290773	837.666181	11.296717
10.492973	835.577864	11.301735
10.239547	837.876342	11.306752
10.224743	852.074416	11.311770
10.242322	849.270484	11.316787
10.352876	874.213196	11.321805
10.518337	864.459128	11.326823
10.796766	859.179564	11.331840
10.862561	874.251183	11.336858
10.964083	869.329530	11.341875
10.818957	868.177381	11.346893
11.044882	864.281534	11.351911
10.924898	866.353573	11.356928
10.901875	871.946145	11.361946
11.063047	855.451018	11.366963
10.546543	836.320475	11.371981
10.829119	835.446699	11.376999
10.221332	839.607732	11.382016
10.533664	851.394702	11.387034
10.854010	862.207997	11.392051
10.852786	867.792831	11.397069
10.932933	866.862266	11.402087
10.926495	872.690832	11.407104
10.966998	866.899898	11.412122
10.847972	865.285547	11.417139
10.740172	869.155734	11.422157
10.888850	873.186946	11.427175
10.929211	875.108595	11.432192
10.927319	877.558882	11.437210
11.206980	863.234612	11.442227
10.827729	863.149015	11.447245
10.759234	857.078021	11.452263
11.042714	863.130376	11.457280
10.783289	875.153752	11.462298
10.802007	863.127013	11.467315
10.939020	873.984783	11.472333
11.058478	870.440818	11.477351
10.925862	860.544018	11.482368
10.604983	872.358592	11.487386
10.807047	866.490574	11.492403
10.920103	866.426260	11.497421
10.973713	864.863387	11.502439
10.697592	867.089846	11.507456
10.852032	873.556764	11.512474
11.089809	869.252241	11.517491
10.728796	873.598938	11.522509
10.926546	870.118595	11.527527
10.883027	875.977007	11.532544
10.928254	879.459869	11.537562
11.079964	867.250647	11.542579
11.074057	880.250154	11.547597
11.019047	877.039294	11.552615
11.170098	872.847803	11.557632
11.180648	873.037394	11.562650
11.093011	871.561825	11.567667
10.914765	867.470710	11.572685
11.402123	878.722178	11.577703
11.334247	874.743212	11.582720
10.895834	870.337084	11.587738
11.137990	875.669831	11.592755
11.170662	889.719470	11.597773
11.223657	893.875141	11.602791
11.519678	904.377090	11.607808
11.500251	878.517330	11.612826
11.308899	879.766278	11.617843
11.221857	883.770907	11.622861
10.926362	871.640308	11.627879
11.327912	874.913427	11.632896
11.266236	890.416681	11.637914
11.403495	881.758599	11.642931
11.029011	879.395958	11.647949
11.372582	900.804095	11.652967
11.451179	889.777689	11.657984
11.406665	896.506193	11.663002
11.369340	891.384782	11.668019
11.040534	885.219024	11.673037
11.187296	896.778516	11.678055
11.551903	901.150066	11.683072
11.232992	898.974364	11.688090
11.380179	905.902056	11.693107
11.386198	912.000282	11.698125
11.495228	905.912134	11.703143
11.509513	899.805302	11.708160
11.301901	898.250166	11.713178
11.798727	896.115515	11.718195
11.461634	903.938933	11.723213
11.254453	903.965230	11.728231
11.669359	899.765753	11.733248
11.522102	903.596415	11.738266
11.536044	898.486998	11.743283
11.699726	902.277691	11.748301
11.550763	893.857417	11.753319
11.947346	896.045044	11.758336
11.464920	891.480859	11.763354
11.519184	872.498327	11.768371
11.411715	880.173472	11.773389
11.730877	871.723874	11.778407
11.581763	872.466229	11.783424
11.382963	887.551671	11.788442
11.851457	879.210044	11.793459
11.469887	884.231179	11.798477
11.466796	900.303200	11.803495
11.807127	899.981782	11.808512
11.751064	901.236716	11.813530
11.798711	904.880867	11.818547
11.640285	876.341126	11.823565
11.609809	874.402061	11.828583
11.872129	880.929487	11.833600
11.408246	883.525990	11.838618
11.520620	885.930334	11.843635
11.506353	896.442321	11.848653
11.697049	897.589954	11.853671
11.640918	893.204588	11.858688
11.709116	902.721240	11.863706
11.666956	892.483645	11.868723
11.680179	897.077503	11.873741
11.514789	909.398695	11.878759
11.813701	897.813629	11.883776
11.743794	904.090313	11.888794
11.840498	903.119417	11.893811
11.835883	898.369696	11.898829
11.571159	895.768776	11.903847
11.631267	901.749516	11.908864
11.580042	904.448369	11.913882
11.760743	903.191300	11.918899
11.797575	904.078487	11.923917
11.752058	920.940863	11.928935
11.892948	923.850644	11.933952
11.898095	932.066947	11.938970
12.136478	929.239700	11.943987
12.379444	925.848410	11.949005
12.157597	914.434806	11.954023
12.379288	902.758480	11.959040
11.766526	906.634775	11.964058
11.825775	895.571511	11.969075
12.073294	890.387284	11.974093
11.520694	884.147210	11.979111
11.810055	901.389676	11.984128
11.942548	924.838958	11.989146
11.971291	922.030610	11.994163
12.253532	925.495965	11.999181
12.201996	929.941803	12.004199
12.388985	923.306512	12.009216
11.993062	923.273169	12.014234
12.113074	918.413492	12.019251
12.405266	931.049270	12.024269
12.068891	918.002327	12.029287
12.194115	897.428795	12.034304
12.167412	879.563370	12.039322
12.148076	894.565234	12.044339
12.044227	886.864739	12.049357
11.946919	907.220947	12.054375
12.105829	923.346619	12.059392
12.248241	937.351695	12.064410
12.202150	941.682484	12.069427
12.370024	930.668457	12.074445
12.255912	933.891099	12.079463
12.510274	927.431942	12.084480
12.153612	919.439017	12.089498
12.376403	922.209401	12.094515
12.574322	912.733647	12.099533
12.286357	908.333054	12.104551
12.254838	890.586107	12.109568
11.874298	900.267842	12.114586
12.024310	913.126572	12.119603
12.268174	916.830115	12.124621
11.907073	919.710273	12.129639
12.148651	926.080348	12.134656
12.176658	921.674476	12.139674
12.446734	919.323894	12.144691
12.369897	925.891837	12.149709
12.398869	926.405589	12.154727
12.276460	921.301180	12.159744
12.072495	923.312906	12.164762
12.265971	924.395920	12.169779
12.208465	930.868168	12.174797
12.099955	939.642235	12.179815
12.336630	948.654389	12.184832
12.788988	956.628722	12.189850
12.410013	958.832139	12.194867
12.656669	966.283483	12.199885
12.499549	966.392042	12.204903
12.767006	954.290471	12.209920
12.579102	959.085075	12.214938
12.854493	962.241979	12.219955
12.524495	944.318154	12.224973
12.587141	943.103520	12.229991
12.592430	935.950710	12.235008
12.377155	928.456565	12.240026
12.375446	950.570237	12.245043
12.595415	956.499389	12.250061
12.649380	962.377839	12.255079
12.803474	956.927189	12.260096
12.709381	953.268423	12.265114
12.852305	957.245303	12.270131
12.835898	949.782742	12.275149
12.667344	957.643973	12.280167
12.948063	941.561403	12.285184
12.814005	940.386852	12.290202
12.818190	941.127199	12.295219
12.546950	933.082658	12.300237
12.398311	945.386841	12.305255
13.077403	950.257420	12.310272
12.781699	962.526580	12.315290
12.821599	954.459739	12.320307
13.012718	961.029767	12.325325
12.917492	946.324733	12.330343
12.660078	930.412190	12.335360
12.799041	928.426617	12.340378
12.840049	943.247426	12.345395
13.045938	947.538643	12.350413
12.821496	956.327154	12.355431
13.031202	949.093027	12.360448
12.968675	950.090123	12.365466
12.972179	962.871057	12.370483
12.782496	934.149203	12.375501
12.868110	940.249343	12.380519
12.636423	959.057832	12.385536
12.600960	962.283229	12.390554
12.640033	964.560550	12.395571
12.986432	951.538519	12.400589
12.883853	965.523290	12.405607
12.976973	959.773911	12.410624
13.097071	957.815267	12.415642
12.721957	958.634533	12.420659
13.131389	952.206029	12.425677
12.964385	959.313891	12.430695
12.877583	960.559739	12.435712
13.302173	961.634677	12.440730
12.758892	955.148393	12.445747
12.795031	951.025665	12.450765
12.534162	955.503152	12.455783
13.245974	974.288791	12.460800
13.219475	977.330753	12.465818
13.339147	979.848256	12.470835
13.236651	978.231752	12.475853
13.124925	990.122168	12.480871
13.192622	979.979135	12.485888
13.184302	989.935675	12.490906
13.453121	994.436940	12.495923
13.690845	974.903091	12.500941
13.281222	965.790353	12.505959
12.705604	968.100172	12.510976
12.975638	960.070087	12.515994
13.068403	978.308933	12.521011
13.360558	983.505722	12.526029
13.594084	987.242185	12.531047
13.679827	988.044241	12.536064
13.746009	977.324790	12.541082
13.143798	949.732407	12.546099
13.235117	952.614664	12.551117
13.141412	981.230026	12.556135
13.581987	977.707563	12.561152
13.533720	986.771354	12.566170
13.411238	976.830882	12.571187
13.381624	951.890532	12.576205
13.351737	969.478496	12.581223
13.486451	972.334987	12.586240
13.402421	977.038231	12.591258
13.515954	991.729012	12.596275
13.302342	972.620378	12.601293
13.487240	973.143692	12.606311
13.764730	979.820988	12.611328
13.823785	979.582954	12.616346
13.526496	965.059397	12.621363
13.329277	946.000243	12.626381
13.249144	965.217770	12.631399
13.384723	968.360189	12.636416
13.654050	988.842597	12.641434
13.649852	996.062918	12.646451
14.084309	977.084739	12.651469
13.535416	979.896648	12.656487
13.482229	998.647740	12.661504
13.346509	984.677580	12.666522
13.489645	982.112672	12.671539
13.825617	980.583525	12.676557
13.586938	987.650597	12.681575
13.530607	991.225155	12.686592
13.708079	979.229659	12.691610
13.428501	987.645084	12.696627
13.534531	980.520676	12.701645
13.555893	982.833697	12.706663
13.135239	989.001084	12.711680
13.337643	995.064134	12.716698
13.272897	1005.166697	12.721715
13.945732	1007.876404	12.726733
13.911203	1016.384298	12.731751
13.833261	1014.097019	12.736768
13.890135	1009.345565	12.741786
13.712710	1018.840882	12.746803
13.861910	1002.621348	12.751821
13.753293	1020.011590	12.756839
13.780531	1010.389406	12.761856
13.960224	1009.547580	12.766874
13.540584	1012.579825	12.771891
13.605970	1013.118856	12.776909
13.489269	1015.477134	12.781927
13.702886	1020.822816	12.786944
13.800941	1025.782943	12.791962
13.838119	1047.524446	12.796979
14.136031	1050.381242	12.801997
14.456563	1044.170407	12.807015
14.272881	1036.823620	12.812032
14.079737	1019.086603	12.817050
14.105504	1013.129967	12.822067
14.075827	1016.998401	12.827085
14.033499	1011.480898	12.832103
13.891394	1013.565174	12.837120
13.841070	1009.632574	12.842138
13.939921	1022.001413	12.847155
14.041688	1029.154149	12.852173
14.206480	1037.647421	12.857191
14.205165	1039.861754	12.862208
14.795798	1039.501529	12.867226
14.179271	1031.201155	12.872243
14.003346	1008.591382	12.877261
14.231096	1016.773011	12.882279
14.698276	1021.442158	12.887296
14.461385	1001.070036	12.892314
14.357388	1013.852638	12.897331
14.604881	1010.467471	12.902349
14.647491	1019.191812	12.907367
14.103840	1015.334436	12.912384
14.453820	1006.941571	12.917402
14.502764	1016.757094	12.922419
14.301313	1001.715489	12.927437
14.491437	1001.819116	12.932455
14.339981	1011.052112	12.937472
14.654598	1009.337055	12.942490
14.114392	1013.979892	12.947507
14.138241	1010.450218	12.952525
14.326059	1002.880568	12.957543
14.351665	1018.864619	12.962560
14.437079	1013.465941	12.967578
14.252165	1007.506236	12.972595
14.280785	1013.498718	12.977613
14.279865	1014.157840	12.982631
14.209609	1013.784213	12.987648
14.307218	1009.050334	12.992666
14.237092	1028.421083	12.997683
14.483063	1041.540393	13.002701
14.719224	1043.998211	13.007719
14.391951	1045.708239	13.012736
14.682477	1047.634230	13.017754
14.866532	1045.607240	13.022771
14.572639	1051.459955	13.027789
14.848534	1041.893494	13.032807
14.668546	1044.422640	13.037824
14.766527	1038.009354	13.042842
14.914035	1031.215313	13.047859
14.612060	1038.145551	13.052877
14.575060	1011.632581	13.057895
14.701631	1013.428701	13.062912
14.643806	1042.238900	13.067930
14.310989	1052.987659	13.072947
14.518364	1046.098005	13.077965
14.909384	1046.672776	13.082983
14.628928	1041.259366	13.088000
14.577419	1039.443026	13.093018
14.731650	1045.592291	13.098035
14.827346	1042.162628	13.103053
15.359404	1038.508322	13.108071
14.810900	1040.244871	13.113088
14.948722	1044.297997	13.118106
14.686962	1042.303348	13.123123
14.819002	1044.427153	13.128141
15.133128	1033.409353	13.133159
14.707689	1041.873906	13.138176
14.856968	1031.279934	13.143194
15.107498	1045.308769	13.148211
14.693873	1039.543021	13.153229
15.054620	1034.619219	13.158247
14.941414	1042.051046	13.163264
14.646757	1030.874741	13.168282
14.668159	1039.667941	13.173299
14.644682	1033.664622	13.178317
15.236691	1039.199016	13.183335
14.696360	1042.590819	13.188352
15.136670	1036.924564	13.193370
15.064621	1044.052300	13.198387
14.980371	1043.346298	13.203405
15.342713	1040.792491	13.208423
15.044245	1051.820365	13.213440
15.112751	1029.126574	13.218458
14.745668	1043.934322	13.223475
15.094540	1058.916732	13.228493
15.245327	1062.469479	13.233511
15.395237	1068.787254	13.238528
15.197086	1057.995602	13.243546
15.031271	1056.758192	13.248563
15.339746	1068.180182	13.253581
15.449588	1046.668012	13.258599
15.215211	1059.497784	13.263616
15.151551	1065.401912	13.268634
15.281159	1058.290302	13.273651
15.020516	1071.672165	13.278669
14.999407	1061.920954	13.283687
15.156720	1068.347132	13.288704
15.015825	1066.203985	13.293722
15.145028	1072.467122	13.298739
15.127146	1061.814350	13.303757
14.995215	1073.369545	13.308775
15.069084	1075.731078	13.313792
15.169389	1086.056573	13.318810
15.639440	1099.938473	13.323827
15.613632	1091.404546	13.328845
15.779436	1088.796020	13.333863
15.695939	1082.321087	13.338880
15.446704	1065.973661	13.343898
15.706410	1064.985168	13.348915
15.241213	1062.697025	13.353933
15.553701	1054.639604	13.358951
15.533975	1071.348006	13.363968
15.382547	1069.528788	13.368986
15.712118	1078.183600	13.374003
15.709729	1099.572623	13.379021
15.804823	1076.158446	13.384039
15.404535	1073.474208	13.389056
15.610316	1074.742668	13.394074
15.928623	1075.258602	13.399091
15.590771	1069.065234	13.404109
15.305321	1070.898843	13.409127
15.523668	1086.311245	13.414144
15.606144	1093.180632	13.419162
15.844572	1091.248570	13.424179
15.669512	1099.231992	13.429197
15.889863	1100.281547	13.434215
16.022535	1091.878097	13.439232
15.984583	1100.467889	13.444250
16.220194	1099.135600	13.449267
15.658730	1089.078064	13.454285
15.674003	1082.590745	13.459303
15.924988	1094.496388	13.464320
15.800633	1088.189989	13.469338
15.597511	1099.766022	13.474355
15.577615	1105.245680	13.479373
16.054371	1100.355827	13.484391
16.132708	1101.372758	13.489408
16.059323	1094.413357	13.494426
16.308854	1088.741117	13.499443
15.983600	1093.928574	13.504461
16.176906	1088.575612	13.509479
16.024228	1073.654693	13.514496
16.043087	1068.912750	13.519514
16.090425	1066.485784	13.524531
15.861588	1066.612296	13.529549
16.177087	1074.893511	13.534567
15.846321	1075.510802	13.539584
15.746620	1079.388954	13.544602
15.992577	1093.808386	13.549619
15.930785	1104.061484	13.554637
15.926476	1090.392194	13.559655
15.980329	1093.568120	13.564672
15.909933	1101.382697	13.569690
16.322180	1097.240586	13.574707
15.928978	1107.588407	13.579725
15.961419	1095.667665	13.584743
16.200740	1097.808388	13.589760
16.248178	1091.720997	13.594778
15.883482	1095.250491	13.599795
15.895042	1110.661071	13.604813
16.258723	1110.228525	13.609831
16.296589	1129.492396	13.614848
16.513343	1124.826574	13.619866
16.492028	1126.872994	13.624883
16.329855	1133.357506	13.629901
16.270429	1121.837687	13.634919
16.315405	1135.274202	13.639936
16.125598	1132.098947	13.644954
16.543175	1120.679605	13.649971
16.649889	1124.007995	13.654989
16.100313	1131.192246	13.660007
16.229799	1128.414744	13.665024
16.349404	1129.918082	13.670042
16.666495	1129.088578	13.675059
16.656626	1129.585924	13.680077
16.281697	1135.857408	13.685095
16.377697	1126.384392	13.690112
16.264179	1134.445442	13.695130
16.724833	1126.995282	13.700147
16.575928	1128.211551	13.705165
16.371683	1121.546945	13.710183
16.661705	1130.781061	13.715200
16.641415	1126.329380	13.720218
16.585240	1121.848401	13.725235
16.335656	1124.852861	13.730253
16.632029	1134.993455	13.735271
16.475824	1124.298942	13.740288
16.624360	1136.049331	13.745306
16.802075	1150.491115	13.750323
16.860149	1161.790016	13.755341
16.996439	1158.753946	13.760359
16.847168	1134.681949	13.765376
16.830731	1129.177444	13.770394
16.984150	1125.713227	13.775411
17.009478	1123.613851	13.780429
16.873269	1124.736895	13.785447
16.554828	1124.545593	13.790464
16.848161	1128.125382	13.795482
16.920000	1117.611459	13.800499
16.701275	1130.652447	13.805517
16.875565	1135.766224	13.810535
17.090085	1139.432256	13.815552
16.606747	1146.438863	13.820570
17.102673	1144.094619	13.825587
17.254650	1161.958407	13.830605
17.276278	1152.223103	13.835623
17.025745	1123.641835	13.840640
16.763559	1130.743167	13.845658
16.957415	1118.974639	13.850675
16.923676	1136.654754	13.855693
16.723460	1152.759909	13.860711
17.041898	1147.815311	13.865728
17.010479	1162.619762	13.870746
17.237600	1157.082674	13.875763
17.132092	1156.836699	13.880781
17.266500	1170.532240	13.885799
17.374679	1149.466978	13.890816
17.160248	1161.903446	13.895834
17.259795	1161.573790	13.900851
17.318092	1162.485590	13.905869
17.062352	1157.586472	13.910887
17.541692	1155.007801	13.915904
17.227663	1165.998178	13.920922
17.069521	1160.789475	13.925939
17.418823	1167.949787	13.930957
17.733547	1152.042648	13.935975
17.741823	1145.947930	13.940992
17.839509	1142.217177	13.946010
17.413893	1121.586760	13.951027
17.327992	1124.336453	13.956045
17.292831	1120.879389	13.961063
17.407499	1117.901025	13.966080
17.183740	1118.786216	13.971098
17.578056	1129.053904	13.976115
17.235702	1134.304033	13.981133
17.340700	1139.754405	13.986151
18.115000	1146.848608	13.991168
17.169056	1139.431707	13.996186
17.216527	1138.079923	14.001203
17.475092	1145.682707	14.006221
17.591416	1161.891048	14.011239
17.467747	1155.021608	14.016256
17.630455	1155.830144	14.021274
17.455514	1148.475364	14.026291
17.378213	1149.042309	14.031309
17.548663	1157.424100	14.036327
17.704473	1155.124054	14.041344
17.488019	1163.446577	14.046362
17.570406	1165.985623	14.051379
17.528845	1156.751230	14.056397
17.523769	1146.158281	14.061415
17.863280	1152.998997	14.066432
17.436709	1148.492619	14.071450
17.709648	1152.822904	14.076467
17.808228	1159.064960	14.081485
17.800741	1168.237060	14.086503
18.111934	1167.094998	14.091520
18.025673	1181.236986	14.096538
18.362345	1152.657626	14.101555
18.030495	1152.518531	14.106573
17.959435	1158.306220	14.111591
17.787807	1146.569333	14.116608
17.708672	1154.382232	14.121626
17.805684	1153.427508	14.126643
18.035130	1146.125175	14.131661
17.883536	1155.721409	14.136679
17.999472	1153.374220	14.141696
18.083203	1163.929438	14.146714
17.940143	1161.391621	14.151731
18.220557	1169.553706	14.156749
17.714247	1166.054628	14.161767
18.359354	1168.207622	14.166784
17.881661	1170.005503	14.171802
17.982668	1177.675081	14.176819
17.963987	1170.626106	14.181837
17.718159	1175.114947	14.186855
18.151511	1169.950795	14.191872
17.784625	1168.018376	14.196890
18.310140	1167.591364	14.201907
18.046794	1170.224743	14.206925
18.161005	1172.247198	14.211943
18.336523	1170.238726	14.216960
18.061483	1172.564246	14.221978
18.447764	1162.942663	14.226995
18.391387	1173.923730	14.232013
18.106760	1168.919164	14.237031
18.158402	1164.758095	14.242048
18.327091	1183.465858	14.247066
18.375600	1187.721645	14.252083
18.290960	1192.867995	14.257101
18.304419	1205.560295	14.262119
18.288372	1195.317691	14.267136
18.520747	1208.306046	14.272154
18.599032	1199.672785	14.277171
18.830331	1208.229754	14.282189
18.798964	1202.533037	14.287207
18.527504	1187.787123	14.292224
18.620713	1191.958765	14.297242
18.372262	1181.436517	14.302259
18.445770	1197.109343	14.307277
18.314769	1200.551234	14.312295
18.784959	1202.270024	14.317312
18.768859	1205.189073	14.322330
18.876713	1206.314304	14.327347
19.146684	1210.518935	14.332365
18.450818	1192.546046	14.337383
18.885262	1184.614443	14.342400
18.655369	1176.602500	14.347418
18.722027	1186.064080	14.352435
19.012132	1195.019526	14.357453
18.491144	1187.434164	14.362471
18.914480	1193.619812	14.367488
18.709047	1192.738487	14.372506
18.437348	1191.755532	14.377523
18.873686	1188.132755	14.382541
18.547617	1207.152191	14.387559
18.773953	1193.075856	14.392576
18.645310	1192.146808	14.397594
18.462004	1202.409621	14.402611
18.567690	1191.344473	14.407629
18.224152	1209.870619	14.412647
18.522119	1219.356584	14.417664
18.783244	1228.508343	14.422682
18.771247	1241.641817	14.427699
19.285127	1223.590416	14.432717
18.532560	1225.481159	14.437735
19.001502	1229.252586	14.442752
18.907266	1228.197790	14.447770
18.665120	1227.424875	14.452787
19.214851	1237.213482	14.457805
19.013621	1246.874265	14.462823
19.382934	1259.775085	14.467840
19.526178	1259.286064	14.472858
19.362573	1241.772711	14.477875
19.547478	1231.763958	14.482893
19.014970	1231.102205	14.487911
19.166470	1236.769497	14.492928
19.411580	1229.986106	14.497946
19.086314	1226.249452	14.502963
19.429690	1218.145706	14.507981
19.182838	1235.988887	14.512999
19.260951	1231.603776	14.518016
19.127741	1234.722273	14.523034
19.382945	1257.791901	14.528051
19.948052	1246.040851	14.533069
19.819828	1255.162494	14.538087
19.203747	1232.918388	14.543104
19.235251	1224.970293	14.548122
19.171937	1231.306050	14.553139
19.528172	1236.422269	14.558157
19.204634	1254.476341	14.563175
19.707972	1259.099829	14.568192
19.712518	1256.740919	14.573210
19.656202	1269.861469	14.578227
20.088759	1253.785563	14.583245
19.726784	1252.701596	14.588263
19.452979	1229.859876	14.593280
19.362751	1226.562258	14.598298
19.310731	1250.084154	14.603315
19.417730	1247.719140	14.608333
19.571184	1260.477116	14.613351
19.622104	1249.753602	14.618368
19.690634	1255.422015	14.623386
19.607952	1256.324839	14.628403
20.127366	1252.545429	14.633421
19.352533	1266.470430	14.638439
19.736674	1267.594883	14.643456
19.741985	1256.897402	14.648474
19.592766	1259.861684	14.653491
19.677448	1259.085931	14.658509
19.849659	1257.463169	14.663527
19.864462	1256.155153	14.668544
19.815617	1253.968033	14.673562
20.143925	1275.396338	14.678579
20.101540	1266.452126	14.683597
19.949459	1263.064147	14.688615
20.040053	1270.559732	14.693632
20.474396	1262.308078	14.698650
19.870769	1265.061868	14.703667
20.017551	1264.796637	14.708685
20.113534	1255.034220	14.713703
19.964785	1260.475787	14.718720
20.066764	1265.398636	14.723738
20.221016	1279.820210	14.728755
20.475427	1280.642728	14.733773
20.232702	1277.235872	14.738791
20.102061	1261.621867	14.743808
20.349379	1259.472208	14.748826
20.115362	1262.812060	14.753843
20.213464	1265.312509	14.758861
20.408499	1283.191760	14.763879
20.186753	1276.554975	14.768896
20.146833	1284.294934	14.773914
20.381963	1289.443780	14.778931
20.607814	1275.629024	14.783949
20.222316	1285.456481	14.788967
20.143305	1293.240301	14.793984
20.604810	1287.066890	14.799002
20.446570	1290.297391	14.804019
20.409689	1290.562235	14.809037
20.721677	1292.210345	14.814055
20.536455	1294.365356	14.819072
20.655063	1285.420706	14.824090
20.283703	1288.982245	14.829107
20.652919	1287.835309	14.834125
20.267845	1289.203789	14.839143
20.355470	1290.190856	14.844160
20.544027	1292.837556	14.849178
20.509897	1282.553597	14.854195
20.300082	1283.841351	14.859213
20.656783	1288.735892	14.864231
20.509759	1293.955960	14.869248
20.683107	1288.061038	14.874266
20.615248	1290.592458	14.879283
20.660440	1288.707853	14.884301
20.905275	1292.075454	14.889319
20.580515	1289.322602	14.894336
20.548721	1279.327781	14.899354
20.818430	1288.081566	14.904371
20.534900	1289.543484	14.909389
20.560015	1298.616195	14.914407
20.762287	1321.324251	14.919424
21.144322	1318.145587	14.924442
20.977651	1320.429602	14.929459
21.361325	1323.065321	14.934477
21.181990	1315.820028	14.939495
20.973442	1305.934702	14.944512
20.939785	1311.366321	14.949530
20.547443	1317.841710	14.954547
20.627201	1324.207397	14.959565
21.019660	1329.324944	14.964583
20.731480	1315.976337	14.969600
21.189124	1317.251418	14.974618
20.807136	1324.152197	14.979635
21.207697	1320.982084	14.984653
20.962393	1318.928388	14.989671
20.964891	1319.193614	14.994688
20.897496	1329.636538	14.999706
20.872728	1343.295357	15.004723
20.757281	1346.938419	15.009741
21.182699	1347.106793	15.014759
21.229900	1348.239892	15.019776
21.561257	1348.780251	15.024794
21.315960	1359.796410	15.029811
21.317513	1350.804737	15.034829
21.639444	1347.281329	15.039847
21.475062	1350.245379	15.044864
21.797111	1347.339968	15.049882
21.307165	1347.747192	15.054899
21.734098	1343.867902	15.059917
21.741836	1340.979989	15.064935
21.511259	1346.284345	15.069952
21.749105	1340.460030	15.074970
21.687585	1344.713770	15.079987
21.672486	1339.255616	15.085005
21.805837	1340.519141	15.090023
21.080649	1339.038566	15.095040
21.822068	1337.747061	15.100058
21.814038	1345.190291	15.105075
21.505464	1349.977303	15.110093
21.919384	1348.265187	15.115111
21.461368	1360.598586	15.120128
21.683004	1349.979841	15.125146
21.656786	1349.085227	15.130163
21.507684	1348.041063	15.135181
21.667621	1352.415862	15.140199
21.546165	1352.877924	15.145216
21.952232	1340.409891	15.150234
21.781482	1351.586139	15.155251
21.952571	1354.697477	15.160269
21.742298	1348.701777	15.165287
21.501996	1349.437179	15.170304
21.983604	1344.717485	15.175322
21.586002	1352.299690	15.180339
21.913664	1344.081958	15.185357
21.999694	1349.560928	15.190375
21.871948	1349.820516	15.195392
21.911964	1353.385141	15.200410
21.762411	1376.795218	15.205427
21.967668	1379.348046	15.210445
22.336519	1377.962224	15.215463
22.220110	1391.356744	15.220480
22.396669	1376.769846	15.225498
22.537452	1388.788993	15.230515
22.456287	1365.213768	15.235533
22.398163	1341.189171	15.240551
22.188154	1352.660250	15.245568
22.099748	1344.683687	15.250586
21.957590	1338.222868	15.255603
22.181248	1357.726163	15.260621
22.262988	1371.777778	15.265639
21.974957	1373.676012	15.270656
22.186620	1379.606798	15.275674
22.537125	1381.290475	15.280691
22.138198	1373.648831	15.285709
22.395844	1375.635801	15.290727
22.538029	1378.032344	15.295744
22.328568	1381.493736	15.300762
22.195169	1373.407486	15.305779
22.306400	1378.352657	15.310797
22.463797	1382.747370	15.315815
22.314085	1383.743746	15.320832
22.490930	1384.198043	15.325850
22.317977	1382.118998	15.330867
22.429211	1389.293168	15.335885
22.738465	1403.544187	15.340903
22.516313	1412.513359	15.345920
22.695659	1412.210269	15.350938
22.469093	1411.754014	15.355955
22.672953	1412.118427	15.360973
22.874418	1413.079603	15.365991
22.640196	1411.620432	15.371008
22.643094	1411.439990	15.376026
22.800132	1415.900903	15.381043
22.805822	1412.128014	15.386061
23.097181	1396.060532	15.391079
22.632896	1407.835639	15.396096
22.923957	1404.184663	15.401114
22.809463	1410.210495	15.406131
22.608148	1408.028079	15.411149
22.744436	1407.553587	15.416167
22.708392	1418.037644	15.421184
22.872395	1418.166947	15.426202
22.701588	1430.862721	15.431219
22.638688	1437.207352	15.436237
23.431667	1442.359719	15.441255
23.338499	1440.480443	15.446272
23.254224	1432.147300	15.451290
23.600520	1433.192206	15.456307
23.681049	1433.286294	15.461325
23.247064	1407.446029	15.466343
23.299321	1417.672617	15.471360
23.402418	1405.428982	15.476378
23.420605	1395.642526	15.481395
23.155216	1405.030194	15.486413
23.300608	1394.272860	15.491431
23.337436	1399.637360	15.496448
23.110277	1403.907663	15.501466
23.397524	1401.091839	15.506483
23.060956	1404.896436	15.511501
23.734659	1411.133896	15.516519
23.224453	1423.563358	15.521536
23.404208	1426.948435	15.526554
23.643040	1427.771961	15.531571
23.297975	1429.133250	15.536589
23.656963	1435.836052	15.541607
23.571492	1442.555817	15.546624
23.273840	1438.288443	15.551642
23.128072	1429.798165	15.556659
23.381629	1434.154367	15.561677
23.768445	1437.620173	15.566695
23.206519	1444.018732	15.571712
23.424857	1433.775420	15.576730
23.787083	1437.325789	15.581747
23.602101	1436.719966	15.586765
23.629037	1430.749001	15.591783
23.815867	1438.889692	15.596800
23.766556	1438.523812	15.601818
23.727147	1440.862985	15.606835
23.753659	1445.107519	15.611853
23.984322	1454.957850	15.616871
23.986874	1458.969767	15.621888
24.107370	1454.505946	15.626906
24.089855	1428.937127	15.631923
23.796439	1444.413791	15.636941
23.927916	1437.032840	15.641959
24.074030	1449.431412	15.646976
24.097657	1452.621658	15.651994
24.159079	1459.172689	15.657011
24.124550	1460.338787	15.662029
24.121058	1454.364379	15.667047
23.943239	1449.924662	15.672064
24.090122	1463.551877	15.677082
24.388626	1459.954374	15.682099
24.141143	1466.458437	15.687117
23.769230	1462.551309	15.692135
23.776946	1465.121246	15.697152
24.169186	1459.414069	15.702170
24.714790	1457.773081	15.707187
24.378153	1458.964697	15.712205
24.442124	1462.131942	15.717223
24.076880	1455.936842	15.722240
24.358489	1453.049116	15.727258
24.499412	1456.723056	15.732275
23.827593	1458.279269	15.737293
24.472284	1461.255681	15.742311
24.868925	1453.987572	15.747328
24.315828	1455.139576	15.752346
24.515869	1452.997703	15.757363
24.264155	1458.414038	15.762381
24.424073	1454.366673	15.767399
24.524801	1469.803422	15.772416
24.516138	1487.458342	15.777434
24.564287	1493.378404	15.782451
24.669197	1496.417058	15.787469
24.791981	1496.943471	15.792487
24.977835	1500.981794	15.797504
25.061400	1492.806682	15.802522
24.817789	1488.497298	15.807539
24.568710	1469.340568	15.812557
24.590498	1476.913363	15.817575
24.952317	1483.637959	15.822592
24.721300	1482.901769	15.827610
25.110302	1492.153599	15.832627
24.755170	1490.577018	15.837645
24.896212	1492.155972	15.842663
25.044867	1485.232329	15.847680
24.602869	1492.585555	15.852698
25.041419	1492.335876	15.857715
24.661856	1489.007679	15.862733
25.044408	1494.951210	15.867751
25.049286	1498.630124	15.872768
24.683500	1480.650178	15.877786
24.751871	1495.018439	15.882803
24.804357	1496.601792	15.887821
24.454738	1498.000055	15.892839
24.886289	1518.245073	15.897856
24.555128	1515.766230	15.902874
25.321789	1521.082203	15.907891
25.058596	1529.690954	15.912909
25.122740	1524.459172	15.917927
25.188331	1515.599911	15.922944
25.071284	1523.735359	15.927962
25.544298	1536.998946	15.932979
25.646785	1545.623250	15.937997
25.400889	1534.404962	15.943015
25.319971	1522.100908	15.948032
25.667252	1538.730471	15.953050
25.621516	1528.319347	15.958067
25.692321	1519.377934	15.963085
25.684243	1520.670357	15.968103
26.055511	1504.147101	15.973120
25.708851	1520.044588	15.978138
25.982106	1516.577408	15.983155
25.730091	1516.863833	15.988173
26.115839	1516.212111	15.993191
25.722020	1512.943736	15.998208
25.432476	1522.708249	16.003226
25.846597	1511.294110	16.008243
25.714162	1512.431517	16.013261
25.618944	1517.486035	16.018279
25.714514	1515.373818	16.023296
25.559435	1504.395233	16.028314
25.832096	1506.931826	16.033331
26.126492	1520.572898	16.038349
25.514587	1506.962704	16.043367
25.841846	1508.618746	16.048384
25.611298	1525.995460	16.053402
26.073600	1534.272347	16.058419
26.153173	1544.751555	16.063437
26.082910	1549.327421	16.068455
26.120964	1546.931831	16.073472
25.814418	1550.708474	16.078490
25.893622	1543.558913	16.083507
25.996148	1543.190377	16.088525
25.817873	1557.147549	16.093543
25.997663	1541.338084	16.098560
25.962337	1544.829389	16.103578
26.092836	1539.889941	16.108595
26.634243	1552.911957	16.113613
26.249707	1544.989344	16.118631
26.335374	1539.694363	16.123648
26.167425	1549.969434	16.128666
26.407488	1546.220567	16.133683
26.325851	1542.342999	16.138701
26.281513	1550.714639	16.143719
26.354416	1562.046417	16.148736
26.646668	1580.212072	16.153754
26.923388	1567.029900	16.158771
26.889262	1559.608943	16.163789
26.402335	1546.166028	16.168807
26.780085	1542.958110	16.173824
26.495154	1550.358036	16.178842
26.473422	1539.793746	16.183859
26.578930	1541.609056	16.188877
26.398868	1553.325102	16.193895
26.867753	1556.895271	16.198912
26.667769	1572.791996	16.203930
27.087383	1567.577235	16.208947
26.809605	1569.244696	16.213965
26.519482	1566.482920	16.218983
26.726094	1562.684467	16.224000
26.694712	1579.344172	16.229018
26.578076	1577.443761	16.234035
26.642066	1564.628786	16.239053
26.677717	1579.276117	16.244071
26.660221	1577.129826	16.249088
26.628515	1580.081048	16.254106
26.671210	1576.877121	16.259123
26.754653	1578.301451	16.264141
26.676433	1609.930262	16.269159
26.894883	1610.530819	16.274176
27.154771	1608.813819	16.279194
27.110926	1616.116857	16.284211
27.281844	1615.348487	16.289229
27.374584	1616.568163	16.294247
27.508332	1599.207600	16.299264
27.492987	1607.203664	16.304282
27.038147	1605.927367	16.309299
27.305765	1605.100898	16.314317
27.254485	1607.239329	16.319335
27.615643	1607.315978	16.324352
27.233809	1607.739195	16.329370
27.356068	1606.510427	16.334387
27.122433	1604.310688	16.339405
27.025227	1602.645220	16.344423
27.181497	1599.979727	16.349440
27.168108	1602.938358	16.354458
27.289558	1612.347254	16.359475
27.529362	1618.566553	16.364493
27.658580	1624.822631	16.369511
27.707697	1628.958377	16.374528
27.521472	1640.120463	16.379546
27.496166	1631.300957	16.384563
27.828825	1629.089316	16.389581
27.630731	1632.070012	16.394599
27.608028	1625.208871	16.399616
27.643925	1627.358879	16.404634
27.644827	1631.159332	16.409651
27.796166	1623.362466	16.414669
27.355904	1631.586220	16.419687
27.488627	1627.424618	16.424704
27.566989	1650.269762	16.429722
27.891312	1653.669577	16.434739
28.141642	1652.874108	16.439757
28.064396	1667.551201	16.444775
28.262421	1661.928990	16.449792
28.245700	1665.148386	16.454810
28.535085	1668.678371	16.459827
28.243217	1658.825087	16.464845
27.989088	1667.093878	16.469863
28.085548	1656.933543	16.474880
28.251218	1661.086843	16.479898
27.943081	1656.899280	16.484915
28.176362	1649.229786	16.489933
28.365242	1659.219418	16.494951
28.614712	1648.720459	16.499968
28.164234	1663.643846	16.504986
28.341581	1659.357948	16.510003
28.436518	1649.113432	16.515021
28.401060	1666.364378	16.520039
28.794078	1647.527837	16.525056
28.345296	1658.126713	16.530074
28.294903	1660.035901	16.535091
28.875828	1655.153068	16.540109
28.482338	1661.906508	16.545127
28.306583	1652.416864	16.550144
28.381842	1656.669540	16.555162
28.383277	1652.163731	16.560179
28.620922	1651.764794	16.565197
28.394604	1663.365946	16.570215
28.451497	1651.891067	16.575232
28.482741	1651.360118	16.580250
28.707533	1675.699207	16.585267
29.073470	1668.061319	16.590285
28.891716	1676.276035	16.595303
29.151825	1661.623296	16.600320
29.081318	1647.422200	16.605338
28.854201	1653.372262	16.610355
29.149223	1652.670378	16.615373
28.721529	1653.332247	16.620391
28.884316	1652.440826	16.625408
29.174119	1647.202613	16.630426
29.009097	1659.740751	16.635443
29.504127	1653.702189	16.640461
29.164008	1651.859168	16.645479
28.935869	1648.509653	16.650496
29.057275	1651.764873	16.655514
28.755883	1666.072366	16.660531
29.069319	1672.410211	16.665549
29.045384	1678.264707	16.670567
29.282210	1676.555054	16.675584
29.005648	1672.224688	16.680602
28.936629	1669.330896	16.685619
29.363680	1682.690776	16.690637
29.104772	1689.901453	16.695655
29.036220	1673.695350	16.700672
29.372066	1695.696739	16.705690
29.347504	1708.564022	16.710707
29.362686	1701.258651	16.715725
29.494362	1713.842475	16.720743
29.412531	1709.778897	16.725760
29.755825	1702.468117	16.730778
29.445930	1716.414314	16.735795
29.749000	1709.423326	16.740813
29.557216	1715.921832	16.745831
29.711520	1706.665764	16.750848
29.899738	1706.014595	16.755866
29.539746	1719.125677	16.760883
29.873973	1700.185220	16.765901
29.920247	1703.205459	16.770919
29.943642	1706.590456	16.775936
30.328934	1702.177281	16.780954
30.160008	1709.778557	16.785971
30.089732	1700.491503	16.790989
29.841900	1707.033318	16.796007
30.017612	1712.247630	16.801024
29.923992	1706.421662	16.806042
29.771876	1705.944434	16.811059
30.007716	1707.165663	16.816077
29.787688	1703.490624	16.821095
29.861635	1702.712293	16.826112
30.080260	1711.670012	16.831130
30.210057	1730.772219	16.836147
30.461542	1736.210405	16.841165
30.554833	1734.362871	16.846183
30.249938	1720.628928	16.851200
30.650574	1709.082048	16.856218
30.051242	1716.761931	16.861235
30.464976	1709.459584	16.866253
30.484341	1729.798188	16.871271
30.663391	1727.244052	16.876288
30.533805	1720.231261	16.881306
30.393261	1709.238711	16.886323
30.167468	1702.331185	16.891341
30.573303	1726.462311	16.896359
30.543348	1736.014595	16.901376
30.639363	1734.666940	16.906394
30.399426	1748.869287	16.911411
30.490752	1732.131059	16.916429
30.788379	1736.419639	16.921447
30.366311	1729.988770	16.926464
30.494322	1731.853527	16.931482
30.445485	1742.093887	16.936499
30.394814	1730.702267	16.941517
30.369615	1750.119248	16.946535
30.429265	1756.963968	16.951552
30.419222	1769.530514	16.956570
30.528800	1768.213485	16.961587
30.875100	1765.764759	16.966605
31.126800	1766.890076	16.971623
30.731328	1767.224814	16.976640
31.041065	1768.643063	16.981658
30.894419	1788.594072	16.986675
31.273925	1796.779088	16.991693
31.750734	1790.597833	16.996711
31.603515	1780.944358	17.001728
31.586806	1769.307955	17.006746
31.148802	1757.502823	17.011763
31.550282	1744.840170	17.016781
31.321196	1762.384407	17.021799
31.298864	1763.097192	17.026816
31.459264	1745.724187	17.031834
31.342206	1761.847530	17.036851
31.340688	1750.170052	17.041869
31.608914	1751.305038	17.046887
31.475701	1755.050922	17.051904
31.651937	1743.998520	17.056922
31.515555	1758.129046	17.061939
31.693226	1743.625466	17.066957
31.676316	1749.526066	17.071975
31.454782	1754.510405	17.076992
31.672378	1744.129430	17.082010
31.563121	1748.911969	17.087027
31.609987	1762.682535	17.092045
31.649991	1770.895691	17.097063
31.715557	1787.604356	17.102080
32.011100	1785.642104	17.107098
31.654902	1784.222342	17.112115
32.111915	1797.028029	17.117133
32.207899	1777.699340	17.122151
31.949471	1783.380448	17.127168
32.040877	1783.274735	17.132186
31.725575	1783.389164	17.137203
31.693173	1780.374157	17.142221
32.087873	1776.072582	17.147239
31.790082	1779.810634	17.152256
32.063853	1779.245901	17.157274
31.705281	1773.924066	17.162291
31.938461	1787.795739	17.167309
32.204892	1798.511335	17.172327
32.474515	1801.521256	17.177344
32.828334	1814.489859	17.182362
32.449041	1800.514823	17.187379
32.936609	1787.609591	17.192397
32.655139	1775.391224	17.197415
32.409613	1771.255677	17.202432
32.555607	1761.192783	17.207450
32.419342	1770.359360	17.212467
32.641389	1768.711580	17.217485
32.673856	1761.860943	17.222503
32.570516	1769.004812	17.227520
32.559983	1755.191491	17.232538
32.884188	1766.601956	17.237555
32.497310	1763.481967	17.242573
32.849086	1764.707268	17.247591
32.849799	1768.795348	17.252608
33.121260	1753.065584	17.257626
32.683151	1765.824504	17.262643
32.826337	1767.196466	17.267661
33.174376	1754.460952	17.272679
33.163885	1763.397909	17.277696
32.984139	1758.034522	17.282714
32.833038	1762.556692	17.287731
32.896596	1770.181776	17.292749
33.083409	1765.920659	17.297767
32.946426	1772.984077	17.302784
33.122204	1761.988817	17.307802
33.011494	1763.705649	17.312819
32.781477	1765.267022	17.317837
32.789108	1769.721433	17.322855
32.930179	1789.454644	17.327872
33.076139	1801.302610	17.332890
33.148705	1795.120643	17.337907
33.251219	1797.809009	17.342925
33.355555	1797.417729	17.347943
32.941992	1804.892963	17.352960
33.254665	1804.579053	17.357978
33.347170	1798.342221	17.362995
33.105376	1803.067358	17.368013
33.524751	1818.022917	17.373031
33.311344	1830.951819	17.378048
33.466804	1826.490774	17.383066
33.709173	1822.614310	17.388083
33.678910	1831.833280	17.393101
33.916405	1829.119487	17.398119
33.637671	1826.952953	17.403136
33.451992	1829.938721	17.408154
33.640682	1823.152782	17.413171
33.586684	1824.141045	17.418189
33.375167	1822.718627	17.423207
33.760033	1823.589688	17.428224
33.801249	1839.221660	17.433242
34.196464	1856.322131	17.438259
34.259565	1855.069461	17.443277
34.386541	1836.968894	17.448295
34.169825	1826.031363	17.453312
34.114184	1818.340247	17.458330
34.208805	1816.714306	17.463347
33.968059	1821.445968	17.468365
34.224092	1821.438035	17.473383
33.936378	1828.089432	17.478400
34.071670	1851.954279	17.483418
34.600270	1849.958625	17.488435
34.538864	1851.799192	17.493453
34.668654	1843.474344	17.498471
34.024199	1856.000540	17.503488
34.454403	1858.380662	17.508506
34.547800	1850.314156	17.513523
34.528073	1857.769407	17.518541
34.863172	1855.550247	17.523559
34.540051	1848.520172	17.528576
34.587992	1856.035885	17.533594
34.590672	1853.314834	17.538611
34.555118	1847.416429	17.543629
34.817944	1845.093085	17.548647
35.183525	1849.023069	17.553664
35.096486	1837.688949	17.558682
34.914310	1817.495657	17.563699
34.832824	1810.670324	17.568717
34.618516	1800.711624	17.573735
34.705564	1816.464329	17.578752
34.438991	1830.969739	17.583770
34.816545	1839.572176	17.588787
34.703074	1838.611647	17.593805
34.994065	1835.575468	17.598823
34.697259	1839.408241	17.603840
34.612628	1838.306938	17.608858
35.079026	1839.457602	17.613875
34.854113	1852.426215	17.618893
35.482841	1852.370276	17.623911
35.356822	1862.282368	17.628928
35.586135	1864.151462	17.633946
35.483226	1843.197882	17.638963
35.177104	1836.413989	17.643981
35.678163	1835.627073	17.648999
35.169364	1841.565297	17.654016
35.190479	1842.980466	17.659034
35.368692	1858.453024	17.664051
35.329603	1860.144844	17.669069
35.625434	1863.499027	17.674087
35.307425	1865.951026	17.679104
35.498677	1868.368472	17.684122
35.762178	1862.792448	17.689139
35.674578	1860.923222	17.694157
35.938517	1868.085176	17.699175
35.610954	1867.143489	17.704192
35.940310	1854.802076	17.709210
36.155987	1860.580436	17.714227
35.868710	1857.311504	17.719245
36.090681	1858.978489	17.724263
35.814041	1860.972327	17.729280
36.147496	1847.527225	17.734298
36.123675	1854.165533	17.739315
35.748038	1865.593307	17.744333
36.111578	1855.067681	17.749351
35.920446	1865.035018	17.754368
35.934406	1855.274360	17.759386
35.974158	1860.042546	17.764403
35.846508	1865.884334	17.769421
36.172318	1883.488569	17.774439
36.033930	1890.602661	17.779456
36.122671	1896.132947	17.784474
36.605242	1896.238152	17.789491
36.466423	1889.804694	17.794509
36.039355	1889.811033	17.799527
36.234015	1897.277918	17.804544
36.390253	1892.280370	17.809562
36.519423	1882.345556	17.814579
36.505038	1892.554538	17.819597
36.498471	1890.440842	17.824615
36.014850	1891.890807	17.829632
36.780526	1914.413734	17.834650
36.649241	1923.849036	17.839667
36.667240	1919.295534	17.844685
36.806347	1922.384718	17.849703
36.574709	1918.895382	17.854720
36.834935	1927.536940	17.859738
37.032430	1916.989111	17.864755
37.158394	1925.315098	17.869773
37.023422	1916.401555	17.874791
37.172930	1926.069952	17.879808
37.301047	1916.455529	17.884826
37.525666	1921.451029	17.889843
37.409675	1920.794812	17.894861
37.052584	1908.904547	17.899879
37.386890	1910.767123	17.904896
37.155046	1908.068283	17.909914
36.770475	1904.787863	17.914931
36.852708	1914.595308	17.919949
37.364577	1920.251722	17.924967
37.255827	1903.519994	17.929984
37.245288	1913.008950	17.935002
37.635399	1911.210365	17.940019
37.384356	1908.561543	17.945037
37.779737	1911.065131	17.950055
37.629931	1915.852848	17.955072
37.351827	1917.508786	17.960090
37.583041	1903.736870	17.965107
37.717661	1912.029926	17.970125
37.595780	1920.458277	17.975143
37.661766	1904.304493	17.980160
37.410294	1924.163368	17.985178
37.858821	1915.866903	17.990195
37.790984	1913.248625	17.995213
37.882343	1935.395275	18.000231
38.269009	1930.523791	18.005248
38.059946	1931.277479	18.010266
38.289196	1910.431892	18.015283
38.066790	1918.320028	18.020301
38.036368	1911.664932	18.025319
38.245030	1904.939625	18.030336
37.863603	1910.295278	18.035354
37.812779	1916.364126	18.040371
37.865640	1936.371128	18.045389
38.196062	1948.588483	18.050407
38.345725	1938.557934	18.055424
38.224372	1947.941221	18.060442
38.285036	1936.660564	18.065459
38.521309	1944.263296	18.070477
38.389908	1947.329673	18.075495
38.504899	1934.309529	18.080512
38.356438	1938.015658	18.085530
38.580897	1943.256045	18.090547
38.524960	1933.457287	18.095565
38.393597	1931.360469	18.100583
38.521789	1937.109422	18.105600
38.463058	1948.297508	18.110618
38.927699	1959.784308	18.115635
38.811920	1961.199474	18.120653
39.087785	1963.859813	18.125671
38.841917	1952.729000	18.130688
38.807177	1965.698758	18.135706
39.162552	1952.556207	18.140723
39.030622	1951.478656	18.145741
39.210575	1951.238441	18.150759
39.219338	1955.574032	18.155776
38.946618	1947.472908	18.160794
39.221582	1949.904876	18.165811
39.275844	1953.111421	18.170829
39.377216	1956.258613	18.175847
39.501223	1958.458077	18.180864
39.274394	1952.941593	18.185882
39.493801	1947.329524	18.190899
39.449692	1953.434674	18.195917
39.596307	1955.682167	18.200935
39.602430	1948.860404	18.205952
39.053605	1956.711763	18.210970
39.101764	1949.540179	18.215987
39.527338	1954.646953	18.221005
39.012834	1952.616988	18.226023
39.120742	1948.893013	18.231040
39.143318	1953.360951	18.236058
39.431337	1969.517955	18.241075
39.425455	1983.119108	18.246093
39.647840	1987.195809	18.251111
39.898205	1978.236662	18.256128
40.259193	1991.854748	18.261146
40.171339	1984.143876	18.266163
39.851105	1982.136325	18.271181
39.995560	1992.443914	18.276199
40.333436	1976.621068	18.281216
40.013186	1982.456346	18.286234
40.434269	1991.658497	18.291251
39.933246	1988.026281	18.296269
39.895821	1996.128349	18.301287
39.964928	1985.938660	18.306304
40.135213	1984.073846	18.311322
40.193275	1986.788486	18.316339
40.150883	1988.058275	18.321357
39.689719	1989.770452	18.326375
40.105433	1994.182096	18.331392
40.083364	2000.079708	18.336410
40.389198	2001.053988	18.341427
40.427074	2007.070423	18.346445
40.266897	2011.772885	18.351463
40.489994	2009.506864	18.356480
40.390389	2003.645358	18.361498
40.378904	2005.313540	18.366515
40.516854	2012.555036	18.371533
40.628474	2027.140441	18.376551
40.752499	2032.344705	18.381568
40.632515	2039.330049	18.386586
40.573091	2027.155096	18.391603
40.808488	2030.666728	18.396621
40.568093	2038.203014	18.401639
40.813091	2025.571108	18.406656
40.856161	2035.045768	18.411674
40.749501	2033.810902	18.416691
41.260424	2044.747657	18.421709
41.044012	2060.621026	18.426727
41.333813	2054.458367	18.431744
41.337936	2057.049860	18.436762
41.556967	2060.148696	18.441779
41.595456	2055.664005	18.446797
41.466381	2064.616599	18.451815
41.862075	2059.480028	18.456832
41.460611	2035.189663	18.461850
42.148568	2029.514505	18.466867
42.466465	2015.887202	18.471885
42.365936	2006.477811	18.476903
42.168607	2004.763496	18.481920
42.055121	2012.432522	18.486938
42.212728	1987.976822	18.491955
42.242257	1980.953561	18.496973
41.852449	1967.562132	18.501991
42.185488	1963.380526	18.507008
41.623077	1975.051031	18.512026
42.119291	1966.475627	18.517043
42.173085	1960.499822	18.522061
42.060100	1973.314426	18.527079
42.294410	1958.370820	18.532096
42.090706	1966.475747	18.537114
42.030295	1971.271541	18.542131
42.287276	1959.473835	18.547149
42.160309	1976.081268	18.552167
41.996923	1966.177818	18.557184
41.964661	1963.106459	18.562202
42.182291	1977.903605	18.567219
42.123628	1976.541337	18.572237
42.031892	1993.218549	18.577255
42.251979	1993.442712	18.582272
42.522758	1994.725507	18.587290
42.559289	1997.195506	18.592307
42.584155	1999.151546	18.597325
42.524831	2001.981245	18.602343
42.399309	1997.890759	18.607360
42.307536	2005.052115	18.612378
42.279523	2009.424109	18.617395
42.510902	2007.538568	18.622413
42.440178	2025.406896	18.627431
42.622632	2029.520716	18.632448
43.016883	2028.009199	18.637466
43.008220	2027.953875	18.642483
42.901431	2030.103703	18.647501
42.714601	2040.562515	18.652519
43.099353	2040.520321	18.657536
42.938924	2029.166892	18.662554
42.775297	2034.625361	18.667571
43.091448	2031.781816	18.672589
42.885712	2032.592826	18.677607
42.889790	2048.495095	18.682624
43.136241	2055.525198	18.687642
43.134295	2072.894670	18.692659
43.436370	2065.054564	18.697677
43.247879	2073.880185	18.702695
43.277592	2060.833873	18.707712
43.410460	2059.821599	18.712730
43.189675	2053.118774	18.717747
43.536273	2078.656747	18.722765
43.447344	2088.049523	18.727783
43.515492	2080.908430	18.732800
43.475219	2087.742450	18.737818
43.626522	2093.582711	18.742835
43.786678	2089.200136	18.747853
43.516379	2101.512157	18.752871
43.601804	2089.415964	18.757888
43.757630	2098.933835	18.762906
43.642027	2119.861144	18.767923
44.181471	2116.159115	18.772941
43.852570	2115.464852	18.777959
43.958016	2122.655871	18.782976
44.175849	2117.045182	18.787994
44.366566	2108.801255	18.793011
44.865286	2111.598398	18.798029
44.447103	2103.376362	18.803047
44.761631	2107.942542	18.808064
44.971501	2096.209991	18.813082
44.658495	2107.010727	18.818099
44.604844	2100.766039	18.823117
44.507946	2106.913434	18.828135
44.958235	2102.994276	18.833152
44.719456	2098.979952	18.838170
44.978886	2082.520028	18.843187
44.819583	2074.722502	18.848205
44.660583	2073.646659	18.853223
44.547510	2079.571150	18.858240
44.921751	2086.844886	18.863258
45.116355	2094.571888	18.868275
45.131895	2097.894300	18.873293
45.008143	2105.957351	18.878311
44.949876	2099.844908	18.883328
44.987682	2105.970043	18.888346
44.988248	2104.216520	18.893363
45.008808	2095.464356	18.898381
44.894288	2096.402211	18.903399
45.202934	2085.470584	18.908416
44.899759	2089.831974	18.913434
44.900277	2104.904464	18.918451
44.772503	2093.533781	18.923469
44.887660	2108.508796	18.928487
45.689938	2132.118993	18.933504
45.343079	2132.462237	18.938522
45.166184	2139.670396	18.943539
45.319554	2129.776695	18.948557
45.216306	2137.727921	18.953575
45.317019	2139.645069	18.958592
45.707157	2144.376109	18.963610
45.671951	2163.156352	18.968627
45.701552	2167.671611	18.973645
45.980532	2168.342890	18.978663
46.006459	2171.723831	18.983680
46.118578	2159.392092	18.988698
45.853134	2165.938585	18.993715
46.285953	2155.625695	18.998733
46.161038	2165.130557	19.003751
46.099360	2159.399325	19.008768
46.591179	2150.322234	19.013786
46.393831	2159.798711	19.018803
46.710227	2154.200458	19.023821
46.555352	2154.210827	19.028839
46.593233	2159.265409	19.033856
46.605463	2125.639358	19.038874
46.505827	2121.733715	19.043891
46.658473	2124.426254	19.048909
46.584320	2125.948128	19.053927
46.451946	2112.928752	19.058944
46.855015	2122.642176	19.063962
46.631531	2142.677987	19.068979
46.907551	2153.102708	19.073997
47.137619	2146.670187	19.079015
46.846020	2140.987191	19.084032
47.017056	2125.548812	19.089050
46.933933	2134.599157	19.094067
46.933235	2123.911121	19.099085
47.413589	2136.198132	19.104103
47.113506	2133.635318	19.109120
47.214281	2122.057966	19.114138
47.149704	2121.675302	19.119155
47.456456	2128.138248	19.124173
47.100013	2116.830726	19.129191
46.980360	2127.934924	19.134208
47.319423	2141.606762	19.139226
47.248229	2147.580258	19.144243
47.162716	2138.550944	19.149261
47.446492	2154.458082	19.154279
47.350289	2151.412998	19.159296
47.451787	2146.399613	19.164314
47.304113	2147.305552	19.169331
47.382638	2145.984765	19.174349
47.432484	2150.462228	19.179367
47.356296	2173.415372	19.184384
47.703485	2172.702485	19.189402
48.044132	2172.329819	19.194419
47.784060	2175.518872	19.199437
47.898056	2177.736949	19.204455
47.741820	2175.499340	19.209472
47.810240	2166.832919	19.214490
47.655749	2177.589796	19.219507
48.113201	2190.592178	19.224525
48.138372	2207.085752	19.229543
47.837278	2214.828789	19.234560
48.230214	2201.128496	19.239578
48.098452	2217.655887	19.244595
48.273434	2203.420994	19.249613
48.349884	2192.160768	19.254631
48.258926	2207.337245	19.259648
48.663138	2199.369968	19.264666
48.617734	2198.019071	19.269683
48.602871	2203.367789	19.274701
49.069234	2212.448823	19.279719
48.450806	2189.767142	19.284736
48.604711	2194.702376	19.289754
48.573949	2193.187461	19.294771
48.346361	2194.545738	19.299789
48.719591	2212.300570	19.304807
48.832396	2219.196746	19.309824
49.005787	2219.978381	19.314842
49.166741	2222.372546	19.319859
49.411023	2217.385539	19.324877
49.465324	2215.272960	19.329895
49.393750	2220.065952	19.334912
49.589752	2212.120084	19.339930
49.328047	2221.929841	19.344947
49.303214	2225.151875	19.349965
49.437341	2218.888509	19.354983
49.199338	2222.465029	19.360000
49.247134	2212.495620	19.365018
49.463386	2214.237401	19.370035
49.558553	2212.434968	19.375053
49.275062	2214.725624	19.380071
49.252672	2223.819720	19.385088
49.705838	2212.528327	19.390106
49.408595	2225.282848	19.395123
49.369944	2239.707871	19.400141
49.929573	2241.988920	19.405159
49.860227	2248.830965	19.410176
49.929198	2250.499853	19.415194
49.946369	2245.927103	19.420211
49.904753	2256.227825	19.425229
49.880211	2245.606040	19.430247
49.870523	2256.358726	19.435264
50.040386	2255.307653	19.440282
50.264386	2258.714341	19.445299
50.249109	2282.082148	19.450317
50.677517	2274.160830	19.455335
50.451923	2283.504465	19.460352
50.571324	2284.397378	19.465370
50.696954	2277.926356	19.470387
50.632430	2272.356562	19.475405
50.749640	2275.451797	19.480423
50.791097	2279.396481	19.485440
51.063572	2265.045234	19.490458
50.853397	2267.939276	19.495475
50.670531	2253.232417	19.500493
51.205539	2260.272406	19.505511
51.080280	2264.230464	19.510528
51.043401	2260.334689	19.515546
50.650815	2257.822570	19.520563
50.787890	2263.688670	19.525581
50.762067	2258.837220	19.530599
50.920572	2260.636970	19.535616
51.208584	2257.688990	19.540634
51.142881	2253.425770	19.545651
51.095534	2266.346491	19.550669
51.421107	2256.749617	19.555687
51.205393	2267.238352	19.560704
51.410434	2292.352279	19.565722
51.520684	2296.101956	19.570739
51.651903	2299.512765	19.575757
51.696428	2301.363438	19.580775
51.972857	2295.702257	19.585792
51.833675	2294.746144	19.590810
52.120805	2292.019542	19.595827
51.824979	2294.323073	19.600845
51.681543	2290.718102	19.605863
51.890635	2293.419256	19.610880
51.872398	2285.848879	19.615898
51.628094	2292.902712	19.620915
51.979095	2286.107660	19.625933
51.872025	2295.855300	19.630951
51.938299	2296.824506	19.635968
51.785299	2290.636509	19.640986
52.144067	2296.646089	19.646003
52.155649	2312.029130	19.651021
52.298900	2319.071683	19.656039
52.438183	2320.000089	19.661056
52.297881	2321.537833	19.666074
52.203365	2316.570562	19.671091
52.447667	2316.985201	19.676109
52.411598	2317.444596	19.681127
52.070671	2320.907055	19.686144
52.615342	2330.546822	19.691162
52.780123	2348.210874	19.696179
52.733678	2344.446568	19.701197
53.160905	2332.259454	19.706215
52.948682	2336.178953	19.711232
53.150512	2336.322879	19.716250
53.380257	2342.839582	19.721267
53.524811	2341.845043	19.726285
53.177366	2332.361698	19.731303
53.572057	2343.146236	19.736320
53.845268	2331.196169	19.741338
53.983512	2303.700919	19.746355
53.365525	2300.589090	19.751373
53.545283	2298.113673	19.756391
53.712605	2292.781321	19.761408
53.416411	2297.552799	19.766426
53.554907	2292.972189	19.771443
53.410544	2291.088868	19.776461
53.696151	2289.875569	19.781479
53.563367	2304.593939	19.786496
53.965745	2314.424320	19.791514
53.710550	2322.496410	19.796531
53.819759	2327.347152	19.801549
53.971670	2326.534846	19.806567
53.745704	2330.053107	19.811584
53.795122	2327.044156	19.816602
53.803656	2331.728284	19.821619
53.742640	2329.935900	19.826637
54.098549	2334.379965	19.831655
54.424635	2354.810627	19.836672
54.382577	2355.728452	19.841690
54.321734	2355.428426	19.846707
54.388646	2359.581504	19.851725
54.597518	2346.983650	19.856743
54.199373	2357.987983	19.861760
54.170964	2354.021696	19.866778
54.360032	2349.729144	19.871795
54.323084	2352.477264	19.876813
54.394366	2359.105388	19.881831
54.717090	2378.727652	19.886848
54.576003	2374.908905	19.891866
54.680461	2385.521766	19.896883
54.573332	2388.813137	19.901901
54.630766	2382.116551	19.906919
54.947404	2397.716765	19.911936
54.814814	2412.936934	19.916954
55.332431	2410.287176	19.921971
54.909882	2418.692260	19.926989
55.163674	2401.541648	19.932007
55.036926	2403.761748	19.937024
55.399412	2410.212848	19.942042
55.531494	2397.800855	19.947059
55.426648	2405.610565	19.952077
55.453405	2416.353404	19.957095
55.240115	2415.022356	19.962112
55.672542	2427.678711	19.967130
55.779124	2433.957165	19.972147
55.852471	2431.711892	19.977165
56.211718	2440.839501	19.982183
56.215911	2431.356448	19.987200
55.902472	2432.890532	19.992218
56.175080	2421.381207	19.997235
55.721670	2429.309940	20.002253
56.237249	2428.793804	20.007271
56.180759	2423.652513	20.012288
56.040325	2429.854077	20.017306
56.456479	2436.373478	20.022323
56.312892	2428.999911	20.027341
56.350833	2423.434781	20.032359
56.577994	2432.916271	20.037376
56.563491	2436.761788	20.042394
56.642487	2421.967799	20.047411
56.538663	2428.867191	20.052429
56.447821	2437.796361	20.057447
56.568829	2424.772448	20.062464
56.718675	2429.487383	20.067482
56.840563	2431.564835	20.072499
56.669264	2442.723657	20.077517
56.868479	2445.878204	20.082535
57.170469	2458.306946	20.087552
57.051769	2444.980330	20.092570
57.253340	2447.438876	20.097587
57.283291	2462.437960	20.102605
56.972534	2443.309892	20.107623
57.549400	2451.745104	20.112640
57.228857	2456.218906	20.117658
57.632605	2440.530949	20.122675
57.457159	2448.556465	20.127693
57.320706	2441.384059	20.132711
57.598803	2438.315449	20.137728
57.243574	2439.655866	20.142746
57.825543	2446.265184	20.147763
57.867496	2438.610383	20.152781
58.162598	2447.117741	20.157799
58.017670	2440.976573	20.162816
57.671561	2443.177421	20.167834
57.925891	2451.866308	20.172851
58.157860	2481.031867	20.177869
58.098923	2484.066299	20.182887
58.191410	2478.353170	20.187904
57.927885	2478.931842	20.192922
58.388446	2475.460465	20.197939
58.585281	2477.756426	20.202957
58.184423	2474.347480	20.207975
58.343781	2472.151763	20.212992
58.050650	2471.791899	20.218010
58.400873	2467.471306	20.223027
58.269441	2477.104591	20.228045
58.754468	2485.233370	20.233063
58.852356	2494.635087	20.238080
58.989808	2501.216317	20.243098
59.068645	2497.836752	20.248115
58.953792	2497.028561	20.253133
58.921527	2503.691574	20.258151
59.045449	2498.061819	20.263168
59.003198	2496.078731	20.268186
59.449451	2494.023186	20.273203
59.405502	2493.336537	20.278221
59.158564	2498.461129	20.283239
59.641376	2491.756993	20.288256
59.442337	2492.124238	20.293274
59.256552	2485.814621	20.298291
59.684740	2495.334578	20.303309
59.461971	2489.370217	20.308327
59.578863	2488.647936	20.313344
59.723857	2500.080491	20.318362
59.799650	2484.396687	20.323379
59.427852	2490.569189	20.328397
59.535187	2485.019143	20.333415
59.697314	2486.449649	20.338432
59.722247	2494.690679	20.343450
60.297622	2492.952354	20.348467
59.871269	2487.795000	20.353485
59.890765	2512.252008	20.358503
60.135002	2521.557319	20.363520
59.884957	2527.239871	20.368538
60.116514	2522.088150	20.373555
60.072187	2516.069688	20.378573
60.338136	2518.648503	20.383591
60.439689	2510.689745	20.388608
60.172412	2530.991347	20.393626
60.416811	2537.179948	20.398643
60.288396	2549.737953	20.403661
60.075893	2544.334628	20.408679
60.599953	2555.563257	20.413696
60.174491	2571.872059	20.418714
60.616374	2581.231157	20.423731
60.906427	2582.396063	20.428749
60.659522	2583.157805	20.433767
61.065421	2577.307226	20.438784
61.258624	2570.430654	20.443802
61.223255	2570.305141	20.448819
61.343603	2569.774397	20.453837
61.267805	2576.811733	20.458855
61.558759	2564.165888	20.463872
61.394563	2574.289455	20.468890
61.620429	2592.285204	20.473907
61.848123	2594.904405	20.478925
62.130807	2607.078799	20.483943
62.240395	2588.065133	20.488960
62.022319	2567.644324	20.493978
61.899106	2565.298255	20.498995
61.789795	2559.921570	20.504013
61.896633	2565.498710	20.509031
61.830841	2566.151198	20.514048
62.037989	2582.986335	20.519066
62.163596	2587.574035	20.524083
61.898670	2585.638164	20.529101
62.253669	2583.030406	20.534119
62.323528	2586.233128	20.539136
62.248548	2596.020139	20.544154
62.415395	2589.025875	20.549171
62.504033	2589.626667	20.554189
62.336140	2595.297637	20.559207
62.840033	2580.921241	20.564224
62.343456	2585.294257	20.569242
62.863354	2608.104077	20.574259
63.223168	2606.182872	20.579277
63.116142	2604.522066	20.584295
63.046769	2593.205728	20.589312
62.956230	2586.193569	20.594330
63.268152	2609.122201	20.599347
63.458035	2604.567258	20.604365
63.109010	2596.807509	20.609383
63.537854	2591.943811	20.614400
63.265989	2583.126906	20.619418
63.296109	2596.913976	20.624435
63.320384	2588.917755	20.629453
63.507968	2606.357288	20.634471
63.780412	2590.007265	20.639488
63.766626	2606.328975	20.644506
63.683496	2603.888291	20.649523
63.892551	2606.668832	20.654541
63.678640	2616.317014	20.659559
63.825819	2598.113994	20.664576
63.375703	2608.999937	20.669594
63.516365	2603.384306	20.674611
63.850105	2592.460379	20.679629
63.220976	2605.535784	20.684647
64.193622	2619.283850	20.689664
64.183459	2636.021303	20.694682
64.440511	2630.069325	20.699699
64.507398	2617.989757	20.704717
64.299016	2627.557707	20.709735
64.211414	2627.902800	20.714752
64.200850	2635.033904	20.719770
64.114972	2631.011889	20.724787
64.575741	2643.365728	20.729805
64.533210	2655.368522	20.734823
64.936584	2648.409945	20.739840
65.055829	2643.969215	20.744858
65.151909	2650.849255	20.749875
65.641383	2637.588696	20.754893
65.276915	2641.572403	20.759911
65.743040	2637.837491	20.764928
65.341888	2641.868989	20.769946
65.395877	2645.662101	20.774963
65.524316	2630.961506	20.779981
65.497024	2640.141494	20.784999
65.996991	2643.057619	20.790016
65.802050	2632.736344	20.795034
65.595483	2640.350004	20.800051
65.530209	2633.353529	20.805069
65.600964	2630.731911	20.810087
65.603976	2638.199135	20.815104
65.866778	2640.931630	20.820122
65.423613	2635.214050	20.825139
65.760739	2632.250010	20.830157
65.522836	2640.586319	20.835175
65.610511	2658.128831	20.840192
66.150283	2657.066209	20.845210
65.718996	2664.786696	20.850227
66.050635	2652.743267	20.855245
66.181772	2670.019968	20.860263
66.174328	2685.829134	20.865280
66.255289	2691.043297	20.870298
66.646945	2683.812446	20.875315
66.474547	2686.887908	20.880333
66.371949	2694.313953	20.885351
66.575028	2693.228231	20.890368
67.020071	2697.983243	20.895386
66.984152	2705.871276	20.900403
67.526589	2708.118627	20.905421
67.110077	2708.607634	20.910439
66.956714	2698.798899	20.915456
67.251820	2694.398775	20.920474
67.359225	2716.356506	20.925491
67.388712	2705.093038	20.930509
67.498219	2700.249399	20.935527
67.404151	2709.591241	20.940544
67.621690	2713.885459	20.945562
67.899176	2709.375061	20.950579
67.940375	2705.099365	20.955597
67.717297	2716.821826	20.960615
67.773951	2705.885342	20.965632
67.951677	2708.587028	20.970650
67.937753	2707.883991	20.975667
67.874651	2690.253766	20.980685
67.920649	2710.145197	20.985703
67.927774	2701.805317	20.990720
68.046235	2696.321069	20.995738
67.729557	2707.835972	21.000755
67.967027	2701.720481	21.005773
67.971782	2712.291189	21.010791
68.051965	2721.238125	21.015808
68.469651	2730.746580	21.020826
68.327592	2736.362351	21.025843
68.546760	2729.414887	21.030861
68.373595	2729.658971	21.035879
68.120348	2745.120454	21.040896
68.699165	2755.924264	21.045914
68.841438	2755.214310	21.050931
68.844756	2765.567982	21.055949
68.812902	2762.190116	21.060967
69.093815	2755.840668	21.065984
69.374462	2760.746874	21.071002
69.075129	2752.680034	21.076019
69.439247	2764.044885	21.081037
69.820554	2785.272063	21.086055
69.715116	2767.954435	21.091072
69.590182	2761.825188	21.096090
69.515321	2769.032919	21.101107
69.797152	2766.879518	21.106125
69.952710	2782.744717	21.111143
69.935988	2786.121030	21.116160
70.175072	2781.235484	21.121178
70.029281	2774.950239	21.126195
70.036060	2766.655261	21.131213
69.923036	2784.769041	21.136231
69.937502	2782.222049	21.141248
70.096237	2771.252117	21.146266
70.007601	2785.287705	21.151283
70.247701	2772.956768	21.156301
70.314116	2783.298451	21.161319
70.337153	2790.584891	21.166336
70.558133	2800.841993	21.171354
70.573985	2807.845000	21.176371
70.521070	2797.279293	21.181389
70.661626	2798.854133	21.186407
70.698747	2807.461798	21.191424
70.962111	2803.449741	21.196442
70.896675	2812.653456	21.201459
71.110343	2802.233841	21.206477
71.188820	2816.801653	21.211495
71.175400	2834.642748	21.216512
70.864620	2831.787703	21.221530
71.004936	2838.353250	21.226547
71.102367	2829.788154	21.231565
71.017437	2837.250322	21.236583
71.108599	2863.077658	21.241600
71.691379	2853.688688	21.246618
71.535303	2859.953241	21.251635
71.756615	2868.911980	21.256653
71.532755	2872.554811	21.261671
71.477691	2866.839938	21.266688
71.803205	2878.137634	21.271706
72.243865	2900.406681	21.276723
72.122863	2897.572229	21.281741
72.005144	2901.412476	21.286759
71.943505	2901.351141	21.291776
72.304103	2894.760134	21.296794
72.251010	2894.835961	21.301811
72.250523	2895.796357	21.306829
72.440916	2892.078209	21.311847
72.625551	2899.958832	21.316864
72.829571	2918.043211	21.321882
72.455346	2924.020233	21.326899
72.667461	2932.711643	21.331917
73.117375	2918.302323	21.336935
72.918667	2924.049170	21.341952
73.145135	2920.571106	21.346970
73.145018	2915.542770	21.351987
73.065569	2911.826296	21.357005
73.396859	2911.504766	21.362023
73.191968	2913.052847	21.367040
73.546364	2911.076008	21.372058
73.449951	2916.304794	21.377075
73.483599	2913.419195	21.382093
73.733432	2923.533035	21.387111
73.787911	2936.801055	21.392128
73.797828	2940.508416	21.397146
73.615787	2952.757317	21.402163
73.902061	2934.466945	21.407181
74.016608	2937.472798	21.412199
73.911987	2939.179894	21.417216
74.417059	2930.410776	21.422234
74.291227	2941.435087	21.427251
74.495922	2924.349487	21.432269
74.529367	2941.880221	21.437287
74.192293	2939.436566	21.442304
74.300880	2932.482482	21.447322
74.159011	2933.654028	21.452339
74.455060	2951.142560	21.457357
74.929865	2964.615937	21.462375
74.469378	2963.084755	21.467392
74.675692	2957.590424	21.472410
75.109780	2961.423359	21.477427
74.653081	2959.259298	21.482445
74.874071	2960.093340	21.487463
74.852719	2989.316088	21.492480
75.103819	2982.989190	21.497498
75.349643	2987.052050	21.502515
75.089468	3005.495508	21.507533
75.034529	2994.803234	21.512551
75.350139	3001.008404	21.517568
75.651316	3016.317128	21.522586
75.846700	3018.767931	21.527603
75.728689	3027.515915	21.532621
75.899909	3018.382641	21.537639
76.103171	3022.622221	21.542656
76.137833	3021.871379	21.547674
76.238734	3012.680834	21.552691
76.108260	3022.596964	21.557709
76.149674	3020.873396	21.562727
75.876520	3025.944817	21.567744
76.296727	3041.398063	21.572762
76.604823	3047.023023	21.577779
76.392447	3064.216185	21.582797
76.790116	3042.804258	21.587815
76.820676	3041.247041	21.592832
76.730438	3038.714159	21.597850
76.910263	3042.079308	21.602867
76.799255	3052.504030	21.607885
76.979483	3048.077320	21.612903
76.943128	3036.833938	21.617920
77.209093	3045.812565	21.622938
77.225835	3071.256106	21.627955
77.062872	3072.147694	21.632973
77.621092	3074.947195	21.637991
77.221441	3071.716254	21.643008
77.153427	3074.926703	21.648026
77.230789	3072.357853	21.653043
76.950386	3069.739465	21.658061
77.646132	3087.745939	21.663079
77.868393	3104.695285	21.668096
78.353766	3098.819767	21.673114
78.113886	3102.944413	21.678131
78.305287	3111.114959	21.683149
78.569951	3096.214845	21.688167
78.152103	3111.135017	21.693184
78.790832	3099.198957	21.698202
78.613102	3090.226842	21.703219
78.716149	3102.681892	21.708237
78.696495	3096.933919	21.713255
78.441458	3100.243778	21.718272
78.461994	3099.990523	21.723290
78.749954	3090.329275	21.728307
78.896040	3101.091453	21.733325
78.699770	3089.728007	21.738343
78.671472	3092.768124	21.743360
79.021347	3105.476866	21.748378
78.928738	3091.373561	21.753395
78.935691	3106.593597	21.758413
79.511870	3117.779973	21.763431
79.242412	3115.967218	21.768448
79.126928	3118.968599	21.773466
79.469262	3120.920745	21.778483
79.195810	3118.138607	21.783501
79.470510	3137.986301	21.788519
79.409480	3146.891860	21.793536
79.813449	3151.532546	21.798554
79.756270	3147.901703	21.803571
79.749646	3153.531070	21.808589
79.985329	3152.541501	21.813607
79.985932	3169.404321	21.818624
79.869653	3174.087282	21.823642
80.383351	3184.671848	21.828659
80.123686	3178.073771	21.833677
80.748304	3177.156541	21.838695
80.596236	3183.080022	21.843712
80.649166	3174.282334	21.848730
80.780069	3190.495715	21.853747
80.953320	3209.094164	21.858765
81.411367	3202.822348	21.863783
81.311182	3198.599800	21.868800
80.987080	3200.100287	21.873818
81.069615	3194.323581	21.878835
81.097689	3206.429304	21.883853
81.323494	3200.300586	21.888871
81.142794	3199.014869	21.893888
81.024013	3205.893063	21.898906
81.281059	3208.445909	21.903923
81.424088	3221.448761	21.908941
82.151769	3217.749624	21.913959
81.659612	3226.190659	21.918976
82.161071	3226.121704	21.923994
82.564939	3216.881762	21.929011
82.377693	3221.682367	21.934029
82.392759	3219.663533	21.939047
82.301595	3221.880626	21.944064
82.313676	3216.724589	21.949082
82.549620	3213.908653	21.954099
82.329167	3216.038844	21.959117
82.512936	3210.245404	21.964135
82.331566	3217.794161	21.969152
82.240541	3210.703651	21.974170
82.876464	3215.810343	21.979187
82.598641	3245.655070	21.984205
83.177394	3237.958218	21.989223
83.343348	3238.412406	21.994240
83.087826	3232.551787	21.999258
83.291777	3228.259290	22.004275
83.251451	3240.586179	22.009293
83.504749	3232.544695	22.014311
83.296380	3234.077634	22.019328
83.189069	3238.576068	22.024346
83.594522	3230.448814	22.029363
83.633366	3244.589733	22.034381
84.015620	3231.397174	22.039399
83.902633	3243.377027	22.044416
83.601215	3247.206378	22.049434
83.872361	3236.860042	22.054451
83.969760	3267.453414	22.059469
84.254635	3267.268678	22.064487
83.907526	3268.668645	22.069504
83.800451	3268.180182	22.074522
84.236941	3265.855099	22.079539
84.376159	3277.454731	22.084557
84.078647	3290.365874	22.089575
84.611827	3297.147007	22.094592
84.229766	3293.091480	22.099610
84.524183	3292.334710	22.104627
84.537383	3315.008051	22.109645
84.959529	3306.968155	22.114663
85.142378	3319.011778	22.119680
85.111910	3326.933674	22.124698
85.469244	3319.105263	22.129715
85.166259	3319.400727	22.134733
85.692356	3320.799319	22.139751
85.536458	3313.367915	22.144768
85.692850	3318.736947	22.149786
85.599235	3328.815288	22.154803
85.626280	3328.914882	22.159821
85.573584	3339.554171	22.164839
85.796918	3353.618249	22.169856
85.646620	3349.352366	22.174874
86.269314	3343.561150	22.179891
86.112958	3352.783358	22.184909
86.302819	3366.013234	22.189927
86.418462	3367.371388	22.194944
86.658987	3370.071870	22.199962
86.527344	3366.267063	22.204979
86.608584	3378.734994	22.209997
86.574603	3368.520485	22.215015
86.696052	3371.135921	22.220032
86.505828	3379.324001	22.225050
86.552293	3384.313590	22.230067
86.643565	3399.297151	22.235085
86.821824	3401.700452	22.240103
86.964259	3403.321107	22.245120
87.218907	3418.459182	22.250138
87.379878	3424.553858	22.255155
87.506738	3428.866016	22.260173
87.529399	3434.970560	22.265191
87.750993	3417.521396	22.270208
88.192200	3433.440454	22.275226
88.489588	3421.488507	22.280243
88.229249	3415.732550	22.285261
88.045625	3419.504289	22.290279
88.352464	3411.586541	22.295296
88.358153	3421.541054	22.300314
89.086392	3421.032666	22.305331
88.319903	3414.502487	22.310349
88.561300	3406.151076	22.315367
88.384424	3417.892019	22.320384
88.199403	3418.993567	22.325402
88.697727	3407.106458	22.330419
88.445948	3415.989754	22.335437
88.717168	3437.462787	22.340455
88.823956	3436.439776	22.345472
88.658443	3445.487571	22.350490
88.816958	3442.697380	22.355507
89.201947	3439.741423	22.360525
89.047748	3451.277073	22.365543
89.319837	3463.135593	22.370560
89.180138	3472.492125	22.375578
89.287555	3477.377974	22.380595
89.415548	3477.902220	22.385613
89.305029	3474.167518	22.390631
89.843626	3488.885519	22.395648
89.763186	3502.457415	22.400666
89.952644	3502.740407	22.405683
89.988986	3511.897010	22.410701
90.094607	3508.174221	22.415719
90.538905	3508.885963	22.420736
89.813361	3504.308798	22.425754
90.372943	3511.012830	22.430771
90.652832	3518.398900	22.435789
90.903550	3524.337449	22.440807
90.861226	3532.187000	22.445824
90.663304	3529.689548	22.450842
90.923973	3526.934036	22.455859
90.879908	3522.579686	22.460877
91.040473	3520.677321	22.465895
91.034922	3529.468815	22.470912
90.966082	3543.817956	22.475930
91.571496	3545.725111	22.480947
91.917892	3547.626642	22.485965
91.896951	3557.711626	22.490983
91.782401	3559.442871	22.496000
92.106909	3554.928397	22.501018
92.081475	3555.859885	22.506035
92.011717	3555.800281	22.511053
92.068584	3549.340684	22.516071
92.368805	3553.854937	22.521088
92.061265	3560.554638	22.526106
92.205626	3550.006213	22.531123
92.321575	3560.323301	22.536141
92.189084	3571.841280	22.541159
92.780296	3567.342969	22.546176
92.720752	3575.906798	22.551194
92.764650	3576.966987	22.556211
93.047776	3577.858906	22.561229
92.467767	3589.604389	22.566247
92.924791	3578.385780	22.571264
92.769822	3595.872010	22.576282
93.138564	3609.565445	22.581299
93.028352	3603.766501	22.586317
92.889754	3610.492243	22.591335
93.418550	3616.614798	22.596352
93.371946	3638.929599	22.601370
93.660772	3631.984397	22.606387
93.630884	3625.779259	22.611405
93.489978	3636.478996	22.616423
93.737980	3636.484208	22.621440
93.852809	3657.597562	22.626458
93.889980	3668.054510	22.631475
94.420193	3661.341061	22.636493
94.204797	3663.606302	22.641511
94.691325	3662.594937	22.646528
94.725623	3667.030725	22.651546
94.752843	3652.822069	22.656563
94.750972	3655.719740	22.661581
94.682276	3680.383125	22.666599
95.397734	3679.489443	22.671616
94.947021	3686.207343	22.676634
95.082827	3689.264161	22.681651
95.081115	3692.239766	22.686669
94.965520	3691.083013	22.691687
95.090299	3699.675114	22.696704
95.216191	3695.568223	22.701722
95.420698	3690.614091	22.706739
95.385320	3711.879898	22.711757
95.491416	3711.431787	22.716775
95.653792	3713.335006	22.721792
95.794036	3719.245035	22.726810
95.878110	3712.423787	22.731827
96.045062	3711.862076	22.736845
96.252574	3736.513768	22.741863
96.296436	3748.164549	22.746880
96.573472	3740.894867	22.751898
96.469905	3744.016053	22.756915
96.583427	3743.171043	22.761933
96.393107	3739.518754	22.766951
96.629175	3746.599970	22.771968
96.818818	3760.818410	22.776986
97.016256	3766.897747	22.782003
97.106718	3776.892811	22.787021
97.241040	3773.901834	22.792039
97.446404	3752.171495	22.797056
97.369301	3768.504891	22.802074
97.594435	3761.031177	22.807091
97.615061	3763.837750	22.812109
97.528168	3777.924735	22.817127
98.073628	3764.408299	22.822144
97.713593	3789.658976	22.827162
97.720708	3790.752030	22.832179
98.043253	3789.707124	22.837197
97.739686	3799.628335	22.842215
98.301115	3788.251772	22.847232
97.785014	3802.576631	22.852250
98.231844	3820.071546	22.857267
98.612580	3811.780752	22.862285
98.230452	3834.115054	22.867303
98.824384	3827.281949	22.872320
99.022391	3832.822238	22.877338
98.779674	3852.852410	22.882355
99.067215	3845.791576	22.887373
99.057990	3854.722838	22.892391
99.488565	3847.054505	22.897408
99.421543	3849.069663	22.902426
99.355473	3850.120088	22.907443
99.807265	3844.941187	22.912461
99.083914	3844.800996	22.917479
99.796495	3863.936709	22.922496
99.860038	3876.574502	22.927514
100.086415	3881.427041	22.932531
100.279359	3871.977076	22.937549
100.162716	3878.786315	22.942567
100.273632	3883.330765	22.947584
100.874107	3882.875368	22.952602
100.392753	3884.123159	22.957619
100.286326	3873.380519	22.962637
100.428336	3888.590816	22.967655
100.602298	3898.483971	22.972672
100.853098	3900.011181	22.977690
100.540355	3894.299925	22.982707
100.940357	3905.826620	22.987725
101.206715	3905.650057	22.992743
101.201021	3911.465769	22.997760
101.316089	3922.966723	23.002778
101.174412	3927.325362	23.007795
101.646202	3922.339590	23.012813
101.348929	3933.886641	23.017831
101.864512	3931.340122	23.022848
101.871577	3930.912305	23.027866
101.708242	3926.586605	23.032883
102.084877	3922.925630	23.037901
102.286269	3945.208160	23.042919
102.125680	3943.106445	23.047936
102.563111	3949.800538	23.052954
102.231682	3949.093215	23.057971
102.564541	3946.002469	23.062989
102.155288	3951.323060	23.068007
102.588551	3949.010616	23.073024
102.993585	3955.952196	23.078042
102.385985	3974.657756	23.083059
102.940272	3978.434865	23.088077
103.061726	3979.784240	23.093095
103.135272	3980.460023	23.098112
103.473962	3975.559615	23.103130
103.670707	3980.625747	23.108147
103.673055	3999.954185	23.113165
103.633434	4004.182988	23.118183
104.160662	3997.889975	23.123200
104.209557	3999.365123	23.128218
103.763781	4007.504419	23.133235
103.658267	4002.077390	23.138253
104.359087	4002.990082	23.143271
104.345509	3999.842395	23.148288
104.303396	4007.209071	23.153306
104.293731	4025.745416	23.158323
105.051739	4028.758152	23.163341
104.799520	4037.474942	23.168359
104.949788	4032.678486	23.173376
105.123941	4033.670332	23.178394
104.569388	4042.378812	23.183411
104.824463	4032.809819	23.188429
105.018319	4044.011225	23.193447
105.015990	4055.262379	23.198464
105.253291	4062.409285	23.203482
105.364687	4059.527556	23.208499
105.411559	4070.133569	23.213517
105.607522	4076.867224	23.218535
105.637583	4094.269500	23.223552
105.521072	4093.851469	23.228570
105.434767	4088.527931	23.233587
105.785776	4113.650617	23.238605
105.906896	4116.625692	23.243623
106.224012	4125.108293	23.248640
106.447364	4142.218835	23.253658
106.870295	4154.460451	23.258675
106.737430	4145.301565	23.263693
107.270923	4145.811195	23.268711
107.429800	4140.423503	23.273728
107.637041	4136.935749	23.278746
107.268795	4130.224887	23.283763
107.656120	4126.347919	23.288781
107.717520	4133.297934	23.293799
107.848740	4135.976847	23.298816
108.207883	4128.033165	23.303834
107.822826	4127.318552	23.308851
108.099859	4125.188990	23.313869
108.118406	4121.092638	23.318887
107.936165	4126.567513	23.323904
107.982561	4126.243431	23.328922
107.848084	4121.599908	23.333939
107.866946	4126.921078	23.338957
107.986824	4143.912102	23.343975
108.288136	4148.730689	23.348992
108.766195	4151.195204	23.354010
108.374847	4164.799366	23.359027
108.374979	4155.563771	23.364045
108.978031	4175.828238	23.369063
108.906469	4182.162036	23.374080
109.063118	4172.330867	23.379098
109.077231	4187.401168	23.384115
109.309985	4183.250899	23.389133
109.447380	4178.490779	23.394151
109.300726	4203.627338	23.399168
109.503190	4208.658347	23.404186
109.281101	4209.542445	23.409203
109.696145	4209.802743	23.414221
109.833070	4219.322289	23.419239
110.107620	4240.753363	23.424256
110.392741	4251.275248	23.429274
110.283438	4245.835768	23.434291
110.064160	4237.193092	23.439309
110.415256	4237.617112	23.444327
110.232252	4255.100052	23.449344
110.310481	4255.867597	23.454362
110.093894	4285.284891	23.459379
110.671190	4284.727407	23.464397
111.166892	4299.257592	23.469415
111.041740	4301.390292	23.474432
111.386583	4298.204580	23.479450
111.618465	4304.796174	23.484467
111.793667	4321.608558	23.489485
111.943049	4328.378761	23.494503
111.953762	4336.788874	23.499520
112.262811	4322.713754	23.504538
112.043771	4329.508219	23.509555
112.279451	4314.545587	23.514573
112.282956	4313.445487	23.519591
112.662152	4319.827699	23.524608
112.625765	4323.941088	23.529626
112.382670	4317.381126	23.534643
112.414578	4324.803440	23.539661
112.770506	4337.389750	23.544679
112.718765	4346.250757	23.549696
112.822224	4343.591557	23.554714
112.921298	4348.053057	23.559731
113.086236	4371.000515	23.564749
113.011908	4363.485835	23.569767
113.121800	4388.429900	23.574784
113.456756	4374.052409	23.579802
113.413627	4391.734446	23.584819
113.439175	4403.367876	23.589837
113.827934	4405.478668	23.594855
113.732049	4403.330764	23.599872
113.832137	4428.445024	23.604890
114.147787	4431.188795	23.609907
114.372614	4420.224105	23.614925
114.933231	4426.282275	23.619943
114.973490	4425.363504	23.624960
115.108030	4415.039356	23.629978
115.334847	4427.398637	23.634995
115.088675	4421.343492	23.640013
115.299697	4424.591974	23.645031
115.448141	4425.764479	23.650048
115.481046	4411.086848	23.655066
115.692686	4453.306334	23.660083
115.338723	4459.406579	23.665101
116.050931	4452.715480	23.670119
115.530709	4453.728385	23.675136
115.638127	4468.377615	23.680154
115.856784	4458.621850	23.685171
116.182288	4458.094549	23.690189
116.635665	4476.600591	23.695207
116.212870	4490.256690	23.700224
116.293482	4474.489172	23.705242
116.106160	4493.077083	23.710259
116.279547	4497.003092	23.715277
116.565881	4488.463354	23.720295
116.551705	4501.703502	23.725312
117.112522	4515.291194	23.730330
116.911736	4512.455847	23.735347
116.874627	4518.940397	23.740365
117.102477	4528.621102	23.745383
116.963136	4542.669016	23.750400
117.539730	4548.476943	23.755418
117.331839	4554.331030	23.760435
117.280132	4564.896185	23.765453
117.764814	4577.476377	23.770471
117.564271	4579.699528	23.775488
118.088997	4582.689897	23.780506
118.265566	4598.399144	23.785523
118.495897	4603.683959	23.790541
118.325910	4595.844403	23.795559
118.488916	4613.745400	23.800576
118.936959	4610.334295	23.805594
118.882612	4617.235536	23.810611
119.024783	4630.312156	23.815629
119.429813	4620.880634	23.820647
119.627900	4630.486788	23.825664
119.782525	4618.788633	23.830682
120.222983	4622.244535	23.835699
119.832881	4625.938864	23.840717
120.054520	4618.858255	23.845735
120.086736	4617.994743	23.850752
120.273420	4618.861321	23.855770
120.459507	4604.827526	23.860787
120.105372	4609.897090	23.865805
120.790844	4610.382807	23.870823
120.498936	4616.624837	23.875840
120.430889	4616.668101	23.880858
121.131908	4619.300588	23.885875
120.674149	4637.388443	23.890893
120.837474	4628.472868	23.895911
120.633818	4637.800900	23.900928
121.203881	4642.189779	23.905946
121.604466	4642.693043	23.910963
121.369685	4660.388941	23.915981
121.862931	4659.055129	23.920999
121.990192	4663.278977	23.926016
121.870518	4656.462242	23.931034
122.139524	4664.933403	23.936051
122.006118	4654.657701	23.941069
122.205300	4659.257090	23.946087
122.215819	4660.461066	23.951104
122.194120	4671.052833	23.956122
122.423317	4687.641323	23.961139
122.461229	4687.567467	23.966157
122.704798	4688.128174	23.971175
122.848076	4703.843422	23.976192
122.995965	4709.059214	23.981210
123.078368	4713.887377	23.986227
123.127673	4716.027529	23.991245
123.195101	4714.013631	23.996263
123.619608	4732.393244	24.001280
123.451386	4744.696784	24.006298
123.533893	4734.842076	24.011315
123.488051	4743.860612	24.016333
123.906016	4740.546187	24.021351
123.969537	4751.476313	24.026368
124.003796	4774.017583	24.031386
124.244062	4772.244034	24.036403
124.305383	4774.375909	24.041421
124.607372	4774.702542	24.046439
124.727929	4773.124770	24.051456
124.620488	4788.635451	24.056474
124.960843	4790.853514	24.061491
124.862676	4793.589738	24.066509
125.021129	4797.967141	24.071527
125.043568	4794.519621	24.076544
125.265312	4820.013651	24.081562
125.322178	4829.374740	24.086579
125.430115	4831.914305	24.091597
125.535702	4830.669339	24.096615
125.415183	4849.074182	24.101632
125.607424	4859.885863	24.106650
126.062387	4859.585996	24.111667
126.182587	4883.293625	24.116685
126.549676	4874.863177	24.121703
126.795844	4886.341608	24.126720
126.695822	4885.021942	24.131738
127.406414	4878.138398	24.136755
127.289542	4882.714086	24.141773
127.333358	4877.367203	24.146791
127.052396	4876.425493	24.151808
127.160360	4889.940693	24.156826
127.573965	4906.814325	24.161843
127.040791	4915.904035	24.166861
127.560776	4910.956451	24.171879
127.489875	4923.620851	24.176896
127.652241	4948.254362	24.181914
127.867009	4942.179941	24.186931
128.068593	4945.545850	24.191949
128.188551	4964.673752	24.196967
128.081965	4970.584882	24.201984
128.308058	4964.272342	24.207002
128.773477	4977.035584	24.212019
128.509994	5004.521665	24.217037
129.496191	4997.995320	24.222055
129.608964	4998.797748	24.227072
129.435005	5004.140841	24.232090
129.765385	4993.073263	24.237107
129.631487	4994.867710	24.242125
129.940822	4985.355317	24.247143
129.875234	4985.020192	24.252160
129.882041	5006.694215	24.257178
130.382059	5010.942006	24.262195
130.073776	5009.722889	24.267213
130.357796	5015.580125	24.272231
130.517909	5025.113657	24.277248
130.403984	5018.036343	24.282266
130.388092	5032.758452	24.287283
130.297515	5053.044180	24.292301
130.475898	5037.928106	24.297319
130.836391	5061.694736	24.302336
130.758882	5073.993389	24.307354
131.190949	5077.275175	24.312371
131.180128	5101.075263	24.317389
131.351026	5101.773597	24.322407
131.974334	5110.471129	24.327424
131.860963	5111.334161	24.332442
132.018913	5115.686144	24.337459
132.025102	5130.634638	24.342477
132.148644	5139.069458	24.347495
132.352744	5148.208754	24.352512
132.549360	5140.592232	24.357530
133.122756	5137.120141	24.362547
133.270267	5123.127692	24.367565
133.596226	5119.885483	24.372583
133.680738	5122.643946	24.377600
133.466088	5119.711950	24.382618
133.704613	5104.313802	24.387635
133.415939	5115.040936	24.392653
133.499773	5124.093782	24.397671
133.576434	5130.607034	24.402688
133.719123	5156.328082	24.407706
133.903937	5146.958620	24.412723
133.817261	5152.710215	24.417741
133.959712	5155.644954	24.422759
134.136610	5169.284845	24.427776
134.064574	5181.430695	24.432794
134.385248	5187.476840	24.437811
134.625552	5201.153137	24.442829
134.531593	5214.745294	24.447847
134.686342	5221.876057	24.452864
134.635345	5223.215844	24.457882
135.258302	5238.051899	24.462899
135.099932	5243.873254	24.467917
134.869623	5245.507264	24.472935
135.121916	5270.233127	24.477952
135.334219	5281.158726	24.482970
135.802604	5297.119702	24.487987
135.486756	5308.944483	24.493005
135.717471	5306.500337	24.498023
136.094517	5329.949254	24.503040
136.049813	5344.742171	24.508058
136.621415	5336.023721	24.513075
136.643122	5355.878254	24.518093
136.836450	5365.063950	24.523111
136.963849	5355.049056	24.528128
136.815533	5356.649449	24.533146
137.337854	5373.112668	24.538163
137.392764	5396.619637	24.543181
137.699360	5389.682929	24.548199
138.126063	5384.196614	24.553216
137.924411	5391.096156	24.558234
138.072097	5394.725820	24.563251
138.312523	5407.107255	24.568269
138.242665	5412.597871	24.573287
138.435600	5414.719111	24.578304
138.615719	5424.125159	24.583322
138.535387	5428.402810	24.588339
138.950162	5457.118313	24.593357
138.837329	5456.199185	24.598375
139.263286	5445.303313	24.603392
139.254077	5458.361146	24.608410
139.596582	5458.803163	24.613427
139.643045	5469.727160	24.618445
139.849787	5476.154095	24.623463
140.097401	5474.615502	24.628480
139.919039	5481.346649	24.633498
140.087926	5479.675378	24.638515
140.022534	5491.489625	24.643533
140.200592	5508.651283	24.648551
140.524755	5516.292833	24.653568
140.509535	5510.998013	24.658586
140.500159	5542.986884	24.663603
140.676137	5539.194107	24.668621
140.789140	5536.785914	24.673639
141.116207	5551.524292	24.678656
141.514452	5565.063380	24.683674
141.243155	5569.877801	24.688691
141.420991	5579.874154	24.693709
141.887955	5588.435565	24.698727
142.054887	5581.589181	24.703744
142.192724	5589.449372	24.708762
142.218365	5584.505693	24.713779
142.401410	5586.292724	24.718797
142.686124	5591.610235	24.723815
142.998544	5606.833820	24.728832
143.172874	5613.046062	24.733850
143.299275	5613.808865	24.738867
143.321585	5618.702757	24.743885
143.246278	5613.926160	24.748903
143.292330	5607.593105	24.753920
143.264907	5626.533939	24.758938
143.442218	5606.357425	24.763955
143.501291	5617.971652	24.768973
143.619503	5635.293356	24.773991
143.897749	5630.617017	24.779008
144.066461	5648.695840	24.784026
144.391464	5674.234053	24.789043
144.261475	5663.862228	24.794061
144.680190	5670.664900	24.799079
144.914991	5670.829407	24.804096
145.189251	5675.388736	24.809114
145.031770	5690.864478	24.814131
145.366629	5695.087380	24.819149
145.173187	5691.449714	24.824167
145.543784	5695.646630	24.829184
145.275037	5702.175455	24.834202
145.473259	5712.901296	24.839219
145.535947	5735.005733	24.844237
145.821551	5741.856418	24.849255
146.110685	5739.207646	24.854272
145.908550	5765.184728	24.859290
146.197181	5768.726221	24.864307
146.431339	5779.288275	24.869325
146.752823	5788.612909	24.874343
147.267965	5783.911557	24.879360
146.786856	5793.528278	24.884378
146.966202	5814.019243	24.889395
147.245732	5809.320589	24.894413
147.201844	5836.923439	24.899431
147.544126	5843.476182	24.904448
147.808196	5841.288684	24.909466
147.726134	5850.576476	24.914483
148.210522	5856.234758	24.919501
148.636981	5866.646576	24.924519
148.891661	5869.110088	24.929536
148.821692	5859.913814	24.934554
149.080818	5869.211393	24.939571
149.059583	5863.928866	24.944589
149.153723	5869.993020	24.949607
149.550993	5888.231233	24.954624
149.555222	5909.026099	24.959642
149.364541	5898.964189	24.964659
150.022214	5913.810510	24.969677
149.906180	5902.404580	24.974695
150.043858	5898.861781	24.979712
149.947073	5917.841990	24.984730
149.901325	5926.708414	24.989747
150.158078	5928.907382	24.994765
150.238466	5953.095326	24.999783
150.631179	5956.848438	25.004800
150.852104	5957.774406	25.009818
150.720136	5967.794239	25.014835
151.048213	5976.085070	25.019853
151.206232	5988.342373	25.024871
151.103514	5997.630908	25.029888
151.211746	6010.605614	25.034906
151.434979	6020.009622	25.039923
151.539023	6024.479838	25.044941
151.483610	6051.024576	25.049959
152.069080	6053.941804	25.054976
152.174316	6059.003261	25.059994
152.007253	6071.425777	25.065011
152.791394	6079.556648	25.070029
152.701176	6075.012724	25.075047
153.051204	6085.174679	25.080064
153.105324	6082.107132	25.085082
153.365615	6088.054140	25.090099
153.505565	6106.139425	25.095117
153.633079	6110.975136	25.100135
153.783510	6116.692238	25.105152
153.897146	6116.531836	25.110170
153.916364	6102.962137	25.115187
154.520493	6124.083035	25.120205
154.094678	6139.618124	25.125223
154.543186	6145.544293	25.130240
154.583767	6151.496127	25.135258
154.481738	6146.326477	25.140275
154.588759	6158.105256	25.145293
154.246905	6178.305985	25.150311
154.560091	6182.343989	25.155328
154.858333	6196.094667	25.160346
154.560731	6217.900203	25.165363
155.312378	6229.299250	25.170381
155.364542	6243.886034	25.175399
155.770218	6248.134007	25.180416
155.956995	6266.482649	25.185434
156.439292	6278.379068	25.190451
156.963713	6273.074366	25.195469
156.755217	6297.016823	25.200487
156.579408	6293.624174	25.205504
156.833726	6286.436220	25.210522
156.766643	6317.567556	25.215539
156.844960	6321.588489	25.220557
156.848345	6333.285294	25.225575
157.318210	6360.031211	25.230592
157.685358	6360.712533	25.235610
157.604344	6365.850540	25.240627
157.472530	6382.176803	25.245645
157.673182	6397.866159	25.250663
157.998403	6410.024893	25.255680
158.240513	6433.152817	25.260698
158.548651	6436.868830	25.265715
158.680288	6440.892009	25.270733
158.747075	6463.659903	25.275751
159.232550	6452.711763	25.280768
159.067130	6462.156628	25.285786
159.151277	6489.278363	25.290803
159.944571	6478.800698	25.295821
160.233119	6488.573790	25.300839
160.127769	6508.227899	25.305856
160.247625	6514.776331	25.310874
160.300712	6519.185016	25.315891
160.792477	6514.520390	25.320909
160.869839	6509.772242	25.325927
160.776149	6514.473730	25.330944
160.820341	6526.612835	25.335962
160.805437	6539.516182	25.340979
161.198043	6539.797959	25.345997
161.552393	6553.497154	25.351015
161.605504	6566.333368	25.356032
162.006647	6563.900642	25.361050
162.101593	6572.907205	25.366067
162.177738	6567.927701	25.371085
162.421061	6586.032686	25.376103
162.436271	6587.797556	25.381120
162.661672	6602.242641	25.386138
162.286611	6599.605029	25.391155
163.067730	6612.067403	25.396173
163.302948	6634.791176	25.401191
163.164333	6627.886141	25.406208
163.240003	6639.433409	25.411226
163.342872	6641.385413	25.416243
163.464560	6636.059717	25.421261
163.702573	6644.969440	25.426279
163.674761	6650.286974	25.431296
164.249546	6651.416771	25.436314
163.867365	6674.092191	25.441331
164.147188	6681.925533	25.446349
164.245687	6685.549449	25.451367
164.550478	6706.168518	25.456384
165.098712	6710.968764	25.461402
165.039943	6725.187635	25.466419
164.864582	6726.532740	25.471437
164.839028	6742.959165	25.476455
164.987171	6746.251207	25.481472
165.576058	6772.007106	25.486490
165.333625	6783.803141	25.491507
165.722593	6791.209762	25.496525
165.977289	6804.705913	25.501543
165.962907	6817.616489	25.506560
166.158907	6830.630137	25.511578
166.561991	6839.165382	25.516595
166.667523	6843.312687	25.521613
167.321041	6865.039145	25.526631
167.252787	6868.082659	25.531648
167.529246	6879.105489	25.536666
167.641345	6892.463826	25.541683
167.672657	6900.169800	25.546701
167.797598	6909.241693	25.551719
168.281879	6905.889482	25.556736
168.838221	6905.448797	25.561754
168.827480	6927.691479	25.566771
169.192990	6933.288285	25.571789
169.187300	6933.348421	25.576807
168.967940	6938.121203	25.581824
169.311340	6932.669780	25.586842
169.074508	6940.123954	25.591859
169.429169	6950.503862	25.596877
169.974777	6953.877550	25.601895
170.013546	6968.968111	25.606912
170.091219	6968.064669	25.611930
170.217361	6978.671368	25.616947
170.102657	6984.868119	25.621965
170.172395	6998.383183	25.626983
170.339786	7008.765719	25.632000
170.734090	7011.777725	25.637018
170.869144	7024.051838	25.642035
170.902304	7048.598950	25.647053
171.347684	7044.960950	25.652071
171.087511	7059.992307	25.657088
171.730279	7080.629268	25.662106
171.694251	7093.601926	25.667123
171.623057	7093.910733	25.672141
171.901928	7106.400570	25.677159
172.154717	7128.549588	25.682176
172.691854	7130.081005	25.687194
172.378443	7143.379124	25.692212
172.904880	7146.272452	25.697229
172.921263	7161.431477	25.702247
173.280421	7170.917677	25.707264
173.394409	7182.378679	25.712282
173.367350	7178.249291	25.717300
173.464029	7203.162610	25.722317
173.996596	7207.472576	25.727335
173.951793	7226.077185	25.732352
174.228433	7224.706898	25.737370
174.095186	7243.825467	25.742388
174.196053	7263.670905	25.747405
174.617107	7258.741306	25.752423
174.728873	7278.200622	25.757440
175.162591	7266.540626	25.762458
174.969612	7271.569839	25.767476
175.355081	7290.858722	25.772493
175.721410	7303.861158	25.777511
175.382194	7307.225967	25.782528
175.497715	7316.048412	25.787546
175.720155	7331.972951	25.792564
176.230250	7333.456877	25.797581
176.781471	7351.833204	25.802599
176.587276	7367.483231	25.807616
176.846486	7371.131945	25.812634
176.624227	7378.366544	25.817652
176.905803	7394.913807	25.822669
177.399017	7398.507324	25.827687
177.379928	7402.420976	25.832704
177.867621	7405.279013	25.837722
178.351204	7408.617370	25.842740
178.188936	7416.291787	25.847757
178.687274	7416.918406	25.852775
178.444416	7427.892748	25.857792
179.175825	7431.477633	25.862810
178.888840	7446.394860	25.867828
179.276206	7434.240705	25.872845
179.321049	7445.082464	25.877863
179.173044	7468.351189	25.882880
179.154488	7474.969357	25.887898
179.651528	7488.584360	25.892916
179.959088	7495.312473	25.897933
180.025707	7503.819402	25.902951
180.190151	7522.674897	25.907968
180.064803	7525.506656	25.912986
180.251546	7545.066539	25.918004
180.220262	7565.061781	25.923021
180.358420	7572.963868	25.928039
180.392002	7606.617962	25.933056
180.893675	7617.369394	25.938074
181.294695	7628.447778	25.943092
181.366844	7650.933753	25.948109
181.784848	7657.998895	25.953127
181.794988	7687.408720	25.958144
181.915871	7687.793703	25.963162
182.359411	7697.368667	25.968180
182.088584	7717.337521	25.973197
182.684286	7738.131980	25.978215
182.851710	7749.920872	25.983232
183.254915	7746.837068	25.988250
183.276394	7766.413505	25.993268
183.460692	7774.194654	25.998285
183.517138	7776.560088	26.003303
183.591740	7805.550715	26.008320
184.035863	7805.626320	26.013338
184.319672	7812.742059	26.018356
184.216338	7836.188243	26.023373
184.905389	7840.593035	26.028391
184.935066	7853.018311	26.033408
185.129138	7850.305350	26.038426
185.360931	7859.583816	26.043444
185.186307	7883.255291	26.048461
185.413751	7873.414447	26.053479
185.337206	7899.227794	26.058496
185.532571	7909.726019	26.063514
185.742964	7926.201326	26.068532
185.705723	7938.612522	26.073549
186.425919	7950.292904	26.078567
186.645422	7964.781958	26.083584
186.762341	7981.878444	26.088602
186.922434	7979.709806	26.093620
187.118771	7991.453933	26.098637
187.664643	8000.104053	26.103655
187.788721	8006.194014	26.108672
187.832827	8007.616381	26.113690
188.207985	8019.100998	26.118708
187.888037	8026.609583	26.123725
188.214203	8030.081988	26.128743
188.297521	8043.635872	26.133760
188.555389	8051.741316	26.138778
188.731345	8059.873688	26.143796
188.545897	8061.293819	26.148813
188.831116	8088.642633	26.153831
189.209225	8102.525131	26.158848
189.494329	8109.769172	26.163866
190.000391	8114.552406	26.168884
190.051049	8117.547370	26.173901
190.564554	8114.089267	26.178919
190.759052	8124.794135	26.183936
190.626890	8141.291610	26.188954
191.076149	8120.357302	26.193972
190.937176	8139.828390	26.198989
191.667356	8141.845487	26.204007
191.561040	8167.090011	26.209024
191.259765	8171.049690	26.214042
191.164506	8168.681416	26.219060
190.990411	8190.425155	26.224077
191.151364	8209.796366	26.229095
191.986505	8251.124782	26.234112
192.163274	8259.628883	26.239130
192.535828	8271.080247	26.244148
192.582447	8290.894980	26.249165
192.899159	8298.166179	26.254183
193.269181	8318.726959	26.259200
193.182245	8341.754524	26.264218
193.361980	8347.844085	26.269236
193.344927	8369.589689	26.274253
193.981263	8370.082495	26.279271
194.414404	8390.031974	26.284288
194.865171	8404.519452	26.289306
195.076990	8405.436049	26.294324
194.793170	8405.936750	26.299341
195.541376	8418.675377	26.304359
195.385810	8435.173873	26.309376
195.696042	8434.864398	26.314394
195.524704	8435.335489	26.319412
195.907593	8462.440396	26.324429
196.037480	8464.529940	26.329447
196.165875	8468.719578	26.334464
196.027586	8490.182925	26.339482
196.327167	8502.338850	26.344500
196.534683	8512.652735	26.349517
196.929454	8533.897318	26.354535
196.933073	8540.292515	26.359552
197.222228	8557.547837	26.364570
197.173839	8569.919623	26.369588
197.666302	8586.400999	26.374605
197.917061	8597.634066	26.379623
198.305287	8608.996444	26.384640
198.124325	8625.961683	26.389658
198.409870	8633.357909	26.394676
198.422194	8653.234684	26.399693
198.920544	8653.135933	26.404711
199.017909	8666.814841	26.409728
199.095797	8692.596873	26.414746
199.557353	8693.948754	26.419764
199.799047	8707.423478	26.424781
199.961969	8713.285176	26.429799
200.047167	8721.762910	26.434816
199.879562	8729.667261	26.439834
200.509693	8747.424111	26.444852
200.136313	8766.063550	26.449869
200.804305	8760.793384	26.454887
200.977049	8768.064169	26.459904
201.112949	8790.275788	26.464922
201.326689	8802.667458	26.469940
201.482219	8818.613214	26.474957
201.611675	8827.750051	26.479975
201.924317	8841.054847	26.484992
202.002555	8855.129331	26.490010
202.567057	8877.789325	26.495028
202.677453	8880.991170	26.500045
202.397918	8901.329999	26.505063
203.072519	8910.654858	26.510080
202.834355	8924.846269	26.515098
203.405343	8945.510137	26.520116
203.192417	8959.313029	26.525133
203.530169	8974.661716	26.530151
203.997543	8991.175228	26.535168
204.038125	9013.435201	26.540186
204.673491	9010.987043	26.545204
204.499988	9043.630804	26.550221
204.894700	9043.273492	26.555239
205.460995	9061.316138	26.560256
205.381842	9077.334799	26.565274
205.759123	9079.594645	26.570292
206.066481	9087.182034	26.575309
206.258789	9105.704775	26.580327
206.343019	9108.147736	26.585344
206.552241	9113.502549	26.590362
206.692293	9120.644993	26.595380
206.779011	9136.568568	26.600397
207.213978	9145.180144	26.605415
207.097921	9153.069098	26.610432
207.329963	9167.768278	26.615450
207.630708	9166.693952	26.620468
208.043904	9191.525020	26.625485
207.990247	9205.325440	26.630503
208.456865	9210.546388	26.635520
208.067480	9223.544513	26.640538
208.564360	9239.930531	26.645556
208.507734	9260.625252	26.650573
208.597472	9267.822549	26.655591
209.179292	9289.513787	26.660608
209.168280	9304.343048	26.665626
210.073810	9307.839742	26.670644
210.195128	9319.894993	26.675661
210.395451	9323.565706	26.680679
211.040783	9332.248177	26.685696
210.712470	9359.553255	26.690714
211.103897	9349.500089	26.695732
211.270916	9348.372228	26.700749
211.247799	9375.633211	26.705767
211.599650	9384.979382	26.710784
211.490633	9392.898011	26.715802
211.893199	9414.045601	26.720820
211.835709	9421.994328	26.725837
212.004309	9452.011391	26.730855
212.578271	9452.566532	26.735872
212.601826	9464.053580	26.740890
212.897968	9473.959603	26.745908
213.002385	9483.835082	26.750925
213.338276	9496.286669	26.755943
213.640816	9514.069361	26.760960
213.629752	9522.748535	26.765978
213.979264	9522.868935	26.770996
214.135148	9554.907937	26.776013
214.393132	9556.829162	26.781031
214.489163	9561.364722	26.786048
214.633175	9590.788249	26.791066
214.907649	9572.518122	26.796084
215.100871	9589.512360	26.801101
215.016448	9609.677282	26.806119
215.557437	9620.595306	26.811136
215.501012	9643.219562	26.816154
215.972254	9654.403559	26.821172
216.376222	9664.180033	26.826189
216.622051	9691.232490	26.831207
216.658851	9685.527525	26.836224
216.677787	9704.973649	26.841242
216.757713	9714.905306	26.846260
217.179186	9731.064042	26.851277
217.276104	9743.201627	26.856295
217.408835	9767.521453	26.861312
217.457485	9780.438204	26.866330
217.656563	9809.967255	26.871348
218.278451	9831.852692	26.876365
217.950189	9849.955813	26.881383
218.438496	9861.967382	26.886400
218.620664	9898.591926	26.891418
218.996272	9911.098718	26.896436
219.473032	9925.117757	26.901453
219.259483	9957.243024	26.906471
219.776913	9957.717727	26.911488
219.954163	9977.360162	26.916506
220.023897	9992.353168	26.921524
220.309292	10009.300329	26.926541
220.483185	10031.472743	26.931559
221.184249	10039.468171	26.936576
221.144623	10059.158354	26.941594
221.130640	10083.759698	26.946612
221.626649	10089.705511	26.951629
221.502777	10096.483961	26.956647
221.856114	10131.722728	26.961664
222.043413	10151.955297	26.966682
222.461117	10172.728014	26.971700
222.961160	10183.429477	26.976717
222.852255	10190.209432	26.981735
223.201301	10208.316060	26.986752
223.420661	10229.487914	26.991770
223.777961	10244.513994	26.996788
224.399501	10251.628598	27.001805
224.453682	10265.272689	27.006823
224.945310	10263.178156	27.011840
224.575052	10275.409875	27.016858
224.954628	10297.258791	27.021876
225.763393	10301.189986	27.026893
225.381915	10303.585614	27.031911
225.958499	10318.285649	27.036928
226.069091	10324.408663	27.041946
226.330516	10331.208628	27.046964
226.500736	10347.136947	27.051981
226.680320	10360.057742	27.056999
227.025233	10363.674087	27.062016
226.959580	10378.232151	27.067034
226.680584	10402.966785	27.072052
227.240599	10423.931369	27.077069
227.493427	10441.524013	27.082087
227.851513	10456.491083	27.087104
228.066878	10467.433556	27.092122
228.105410	10462.462200	27.097140
228.784744	10488.735422	27.102157
229.197135	10488.672142	27.107175
229.525766	10486.457992	27.112192
229.369101	10496.270100	27.117210
229.623361	10509.301566	27.122228
230.193042	10518.829833	27.127245
229.852807	10519.260352	27.132263
230.414549	10523.087473	27.137280
230.376114	10545.124741	27.142298
230.427192	10556.446539	27.147316
230.726101	10567.959784	27.152333
230.607702	10591.992292	27.157351
230.835193	10598.942923	27.162368
230.981605	10622.359034	27.167386
231.287022	10649.890098	27.172404
231.519793	10657.468506	27.177421
231.828507	10685.597776	27.182439
232.304078	10697.001576	27.187456
232.522155	10713.588002	27.192474
232.666507	10733.579474	27.197492
232.916050	10740.826658	27.202509
232.996801	10755.750026	27.207527
233.195156	10776.342350	27.212544
233.493970	10792.959634	27.217562
233.723804	10814.418063	27.222580
234.429757	10819.243150	27.227597
234.361953	10840.730308	27.232615
234.932729	10836.804483	27.237632
235.369242	10843.026673	27.242650
235.795175	10871.990046	27.247668
236.442485	10873.512313	27.252685
236.361997	10888.020512	27.257703
236.570218	10878.974270	27.262720
236.750210	10878.516120	27.267738
236.477079	10912.711561	27.272756
236.507341	10917.077976	27.277773
236.329166	10940.463101	27.282791
237.025667	10949.404273	27.287808
237.160622	10984.276880	27.292826
237.350097	10996.608096	27.297844
237.907121	11009.380402	27.302861
238.330006	11018.531463	27.307879
238.269507	11027.990056	27.312896
238.420257	11054.588659	27.317914
238.342856	11065.216751	27.322932
238.717284	11079.579852	27.327949
239.021196	11113.089555	27.332967
239.252463	11128.234187	27.337984
239.555279	11156.536994	27.343002
239.739204	11169.931966	27.348020
239.996089	11178.212483	27.353037
240.256164	11202.106959	27.358055
240.232559	11218.763774	27.363072
240.832404	11227.373664	27.368090
240.811987	11247.666358	27.373108
241.456312	11262.846072	27.378125
241.681509	11285.915330	27.383143
241.777342	11308.826381	27.388160
242.260977	11312.049768	27.393178
242.570919	11318.860259	27.398196
243.186131	11327.522809	27.403213
243.011066	11346.345182	27.408231
243.150927	11360.376244	27.413248
243.385817	11371.797446	27.418266
243.754756	11384.111915	27.423284
244.298389	11401.392086	27.428301
244.435633	11411.241275	27.433319
244.700882	11416.605728	27.438336
245.054832	11437.096779	27.443354
244.635639	11446.728323	27.448372
245.422798	11432.581310	27.453389
245.322081	11448.338847	27.458407
245.437730	11473.497567	27.463424
245.725225	11471.995151	27.468442
246.038501	11495.330612	27.473460
246.228507	11506.871192	27.478477
246.118568	11521.586503	27.483495
246.498397	11544.406852	27.488512
246.772790	11555.888622	27.493530
246.690520	11586.508897	27.498548
246.948122	11600.270197	27.503565
247.428964	11612.540357	27.508583
247.365036	11641.887781	27.513600
247.633982	11669.772467	27.518618
247.620379	11687.408136	27.523636
248.256530	11707.346354	27.528653
248.474045	11737.437617	27.533671
248.834621	11761.481761	27.538688
249.308735	11784.434194	27.543706
249.332074	11789.229767	27.548724
249.925799	11816.269306	27.553741
250.228137	11847.882982	27.558759
250.076054	11840.180642	27.563776
250.918705	11858.932372	27.568794
250.991940	11881.105858	27.573812
251.469629	11886.029649	27.578829
251.844089	11903.904747	27.583847
252.140953	11916.340252	27.588864
251.848227	11917.726444	27.593882
252.003280	11943.097612	27.598900
252.291114	11969.853916	27.603917
252.521991	11977.312728	27.608935
252.871750	12008.175189	27.613952
253.010831	12024.998188	27.618970
253.312414	12047.858966	27.623988
253.383911	12064.519852	27.629005
253.711548	12085.770021	27.634023
253.984652	12111.684453	27.639040
254.118387	12130.379517	27.644058
254.135067	12156.129189	27.649076
254.587949	12166.062986	27.654093
254.795301	12207.093359	27.659111
255.028350	12223.567790	27.664128
255.431197	12240.301742	27.669146
255.544542	12283.820827	27.674164
255.783567	12302.744498	27.679181
256.359401	12313.951689	27.684199
256.369821	12344.075937	27.689216
257.068668	12359.654995	27.694234
257.352010	12367.191982	27.699252
257.603836	12399.155429	27.704269
257.875368	12415.480313	27.709287
258.358841	12416.304211	27.714304
258.526324	12442.183841	27.719322
258.944065	12456.973543	27.724340
259.361327	12451.721558	27.729357
259.747746	12476.747298	27.734375
259.601842	12490.664264	27.739392
259.763765	12486.945831	27.744410
259.580561	12517.117361	27.749428
259.930713	12528.716516	27.754445
260.776435	12553.595587	27.759463
260.812458	12573.046302	27.764480
261.182315	12579.716651	27.769498
261.273939	12601.034855	27.774516
261.632287	12613.961022	27.779533
261.733574	12628.308398	27.784551
261.585977	12655.491523	27.789568
262.238760	12647.755878	27.794586
262.515478	12674.448222	27.799604
262.535198	12693.678028	27.804621
262.804420	12707.764527	27.809639
262.973367	12738.941886	27.814656
263.272209	12747.612571	27.819674
263.546727	12771.091008	27.824692
263.589151	12794.743336	27.829709
264.163517	12819.240633	27.834727
264.078743	12842.460241	27.839744
264.661919	12861.920177	27.844762
264.912824	12874.367955	27.849780
264.939401	12900.942854	27.854797
265.516943	12908.652090	27.859815
265.695771	12932.531046	27.864832
265.857273	12959.337440	27.869850
266.255700	12976.737055	27.874868
266.331114	12996.898728	27.879885
266.496398	13027.881860	27.884903
266.784509	13046.590298	27.889920
267.257615	13064.439359	27.894938
267.579105	13087.377899	27.899956
267.394187	13107.992410	27.904973
268.007960	13134.792131	27.909991
268.292021	13170.505191	27.915008
268.498980	13180.845819	27.920026
268.925559	13190.912233	27.925044
269.323741	13221.636655	27.930061
269.228538	13244.198323	27.935079
269.402001	13261.833957	27.940096
269.905695	13294.703017	27.945114
270.462911	13321.252392	27.950132
270.773889	13330.250719	27.955149
270.837568	13351.738409	27.960167
271.022690	13393.252923	27.965184
271.557656	13406.547640	27.970202
271.659441	13436.607616	27.975220
271.837408	13442.949175	27.980237
272.212612	13461.048064	27.985255
272.562617	13482.977113	27.990272
272.980790	13485.183570	27.995290
273.163062	13520.794461	28.000308
273.531981	13535.319035	28.005325
274.005843	13554.129738	28.010343
274.197657	13568.095835	28.015360
274.416604	13607.418126	28.020378
274.826064	13611.808504	28.025396
274.733789	13630.728586	28.030413
275.198909	13643.138415	28.035431
275.517356	13671.989070	28.040448
275.773920	13680.043229	28.045466
275.904846	13702.223077	28.050484
276.018452	13719.171022	28.055501
276.316027	13744.497049	28.060519
276.573242	13774.095476	28.065536
276.876061	13790.358278	28.070554
277.192288	13815.548966	28.075572
277.508962	13843.257761	28.080589
277.713458	13862.779893	28.085607
278.153276	13878.386673	28.090624
278.545313	13895.129646	28.095642
278.373065	13931.521731	28.100660
278.390306	13947.961089	28.105677
279.287170	13965.323546	28.110695
279.160958	13986.926967	28.115712
279.732977	14003.559950	28.120730
280.088861	14017.404779	28.125748
280.554859	14033.620380	28.130765
281.105638	14028.915496	28.135783
281.171487	14061.825358	28.140800
281.521951	14085.803726	28.145818
281.694658	14086.391471	28.150836
281.795465	14099.887706	28.155853
282.256123	14111.258583	28.160871
281.984385	14139.403900	28.165888
282.352492	14151.034350	28.170906
282.826230	14171.511453	28.175924
282.518425	14200.614641	28.180941
283.189333	14216.193025	28.185959
283.357931	14240.105540	28.190976
283.502125	14274.148529	28.195994
283.772551	14297.330446	28.201012
283.945609	14330.144347	28.206029
284.143937	14353.273644	28.211047
284.511699	14380.614045	28.216064
285.016002	14400.169237	28.221082
285.310571	14432.312438	28.226100
285.889271	14460.108218	28.231117
286.284300	14473.464755	28.236135
286.406216	14498.924987	28.241152
286.599209	14509.687954	28.246170
286.878200	14543.069432	28.251188
287.353685	14563.316664	28.256205
287.670635	14580.731467	28.261223
287.939931	14612.346552	28.266240
287.893733	14628.234488	28.271258
288.422879	14647.875699	28.276276
288.546610	14675.061502	28.281293
288.948928	14704.388663	28.286311
289.560322	14725.652156	28.291328
290.115919	14743.892873	28.296346
290.718552	14742.802203	28.301364
291.262758	14761.689363	28.306381
291.435050	14763.399242	28.311399
291.855112	14773.202970	28.316416
291.999742	14785.827367	28.321434
292.466611	14790.388237	28.326452
292.315130	14798.332289	28.331469
292.725272	14811.344638	28.336487
292.567650	14831.788201	28.341504
292.885483	14850.277914	28.346522
293.498769	14861.343593	28.351540
293.514524	14891.223485	28.356557
293.507832	14912.768991	28.361575
293.975205	14927.759202	28.366592
293.813441	14949.363469	28.371610
294.269892	14971.314767	28.376628
294.116526	15007.999258	28.381645
294.467900	15033.520125	28.386663
295.022288	15064.004753	28.391680
295.065543	15095.043509	28.396698
295.260564	15114.575013	28.401716
295.282925	15147.710157	28.406733
295.959360	15172.091720	28.411751
296.291072	15202.001931	28.416768
296.788209	15229.754193	28.421786
297.253723	15248.692743	28.426804
297.808476	15274.164628	28.431821
298.117843	15297.507011	28.436839
298.161392	15312.443096	28.441856
298.390317	15334.623164	28.446874
298.915085	15367.659993	28.451892
299.247425	15385.601060	28.456909
299.442132	15406.576543	28.461927
299.634255	15430.346660	28.466944
300.441988	15455.572159	28.471962
300.351827	15469.033312	28.476980
300.377233	15490.523846	28.481997
300.932817	15506.923117	28.487015
301.247870	15526.134274	28.492032
301.303869	15545.378796	28.497050
301.174352	15577.080551	28.502068
302.063826	15597.520714	28.507085
302.221897	15620.954746	28.512103
302.910038	15644.903266	28.517120
302.479266	15657.636006	28.522138
303.231448	15682.354112	28.527156
303.106472	15712.607049	28.532173
303.880491	15732.688218	28.537191
304.106444	15764.977767	28.542208
304.051707	15788.845924	28.547226
304.601341	15805.809110	28.552244
304.784911	15837.754357	28.557261
305.031253	15854.495052	28.562279
305.163203	15891.782125	28.567296
305.405115	15926.261580	28.572314
306.078647	15948.395821	28.577332
305.851757	15986.038681	28.582349
306.633939	16009.753134	28.587367
307.570851	16033.951115	28.592384
307.998093	16059.787289	28.597402
308.139182	16072.684343	28.602420
308.489301	16086.728891	28.607437
308.820382	16111.722101	28.612455
308.975356	16132.987189	28.617472
309.150445	16156.537379	28.622490
309.591222	16177.053975	28.627508
309.533094	16199.824794	28.632525
310.119620	16226.282668	28.637543
310.410077	16259.295394	28.642560
310.445962	16277.059467	28.647578
310.758780	16300.643848	28.652596
310.899292	16338.551485	28.657613
311.052043	16361.270354	28.662631
311.442235	16393.395316	28.667648
312.051483	16428.905773	28.672666
312.259867	16452.833870	28.677684
312.287044	16497.856021	28.682701
312.502271	16521.803577	28.687719
313.024522	16553.133187	28.692736
313.392026	16590.075599	28.697754
313.544891	16616.941451	28.702772
314.507355	16641.000569	28.707789
315.026851	16669.481309	28.712807
315.556669	16682.325655	28.717824
315.841603	16698.950512	28.722842
316.756698	16714.413728	28.727860
316.609914	16739.340265	28.732877
317.025471	16752.231912	28.737895
317.569299	16765.433357	28.742912
317.847064	16774.707019	28.747930
317.963768	16776.940101	28.752948
318.328026	16790.210634	28.757965
318.438207	16810.158507	28.762983
318.565305	16824.450155	28.768000
318.816425	16849.006936	28.773018
319.421811	16864.999018	28.778036
319.335637	16886.309650	28.783053
319.711723	16903.718740	28.788071
319.722633	16923.687879	28.793088
320.029352	16961.016283	28.798106
320.480195	16993.335719	28.803124
320.642155	17006.431801	28.808141
320.681109	17039.367861	28.813159
320.974661	17054.138143	28.818176
321.311432	17090.207285	28.823194
321.898476	17116.264602	28.828212
321.955239	17150.026982	28.833229
322.289740	17174.515310	28.838247
322.919629	17194.477088	28.843264
322.837830	17219.863303	28.848282
323.554404	17249.132082	28.853300
323.670141	17277.767268	28.858317
323.917700	17285.036632	28.863335
324.874632	17311.975684	28.868352
324.962460	17340.866198	28.873370
325.555091	17362.155145	28.878388
325.994963	17381.393567	28.883405
326.215356	17400.100857	28.888423
326.403750	17426.854985	28.893440
326.531676	17441.501667	28.898458
326.868755	17461.140170	28.903476
327.463250	17498.155881	28.908493
327.411992	17513.705421	28.913511
327.764263	17528.230005	28.918528
328.017135	17574.128837	28.923546
328.503397	17583.185677	28.928564
328.948239	17611.209110	28.933581
329.112298	17645.750747	28.938599
329.709480	17656.171608	28.943616
330.082663	17691.121697	28.948634
330.311600	17717.510230	28.953652
330.341092	17747.846995	28.958669
330.874245	17778.407966	28.963687
331.529273	17795.812901	28.968704
331.369511	17828.078809	28.973722
331.788418	17843.305101	28.978740
331.922344	17883.550151	28.983757
332.392631	17906.440941	28.988775
332.649645	17925.136472	28.993792
333.077596	17972.856374	28.998810
333.140508	18000.346183	29.003828
333.706473	18024.362505	29.008845
333.813359	18059.708863	29.013863
334.176625	18083.807620	29.018880
334.024796	18132.980886	29.023898
334.919382	18165.606035	29.028916
335.204809	18186.332073	29.033933
335.805919	18229.675305	29.038951
336.405474	18242.610234	29.043968
336.197115	18290.161908	29.048986
336.610729	18310.709302	29.054004
337.423902	18338.681005	29.059021
337.309413	18377.786117	29.064039
338.009653	18399.293490	29.069056
338.222406	18433.917000	29.074074
338.554714	18468.814014	29.079092
338.985490	18492.300087	29.084109
339.177922	18527.825615	29.089127
339.863475	18542.827235	29.094144
339.963338	18568.682032	29.099162
340.495691	18583.401626	29.104180
340.763276	18619.028426	29.109197
341.007222	18643.800287	29.114215
341.598933	18662.575345	29.119232
341.580251	18697.973758	29.124250
341.871839	18726.167845	29.129268
342.501522	18758.224758	29.134285
342.506722	18787.328485	29.139303
342.786482	18810.108562	29.144320
342.694370	18844.876296	29.149338
343.051830	18868.851054	29.154356
343.729090	18902.517661	29.159373
343.499489	18936.526458	29.164391
344.183244	18962.911201	29.169408
344.349180	19003.427961	29.174426
344.942365	19035.333810	29.179444
345.489782	19052.830363	29.184461
345.633864	19097.368973	29.189479
346.010074	19122.037730	29.194496
346.326972	19152.335893	29.199514
346.998039	19170.950246	29.204532
347.287291	19206.692953	29.209549
347.389272	19234.782088	29.214567
348.241281	19258.021536	29.219584
348.224750	19301.031390	29.224602
348.458972	19328.723671	29.229620
348.834738	19351.039376	29.234637
349.176774	19393.610338	29.239655
349.851516	19420.900544	29.244672
349.905591	19460.353951	29.249690
350.418089	19487.303780	29.254708
351.261198	19507.907818	29.259725
351.180264	19545.235164	29.264743
351.979016	19564.635961	29.269760
352.109847	19590.258662	29.274778
352.454478	19611.804293	29.279796
352.987164	19644.785354	29.284813
353.047649	19667.336427	29.289831
353.444956	19693.315663	29.294848
353.771612	19710.130557	29.299866
354.072381	19740.112454	29.304884
354.965420	19777.169075	29.309901
355.101326	19793.668763	29.314919
355.741135	19815.897336	29.319936
355.741565	19852.072206	29.324954
355.791264	19884.252332	29.329972
356.546079	19907.915459	29.334989
356.450364	19949.251756	29.340007
356.848228	19969.444394	29.345024
357.330519	20006.868898	29.350042
357.244361	20047.631628	29.355060
357.837148	20068.384913	29.360077
357.655802	20114.775531	29.365095
358.365029	20150.296400	29.370112
358.753297	20188.712644	29.375130
358.964590	20235.664571	29.380148
359.574064	20266.152895	29.385165
359.989546	20299.788339	29.390183
359.816571	20346.602276	29.395200
360.422473	20378.670979	29.400218
360.835987	20406.340164	29.405236
361.204263	20452.836403	29.410253
361.186084	20490.991011	29.415271
361.820523	20531.784067	29.420288
362.230841	20569.576425	29.425306
362.500382	20615.566045	29.430324
363.344151	20639.102013	29.435341
363.641866	20684.291058	29.440359
363.797882	20715.892427	29.445376
364.429301	20741.935518	29.450394
364.857543	20788.868926	29.455412
365.385805	20818.066358	29.460429
365.079355	20857.045048	29.465447
365.649480	20888.999254	29.470464
366.056030	20920.204914	29.475482
366.432239	20969.409680	29.480500
366.929870	20984.275877	29.485517
367.501251	21020.729433	29.490535
368.029527	21048.000789	29.495552
368.433119	21062.436442	29.500570
368.723472	21089.379846	29.505588
369.651928	21102.473935	29.510605
369.771133	21129.748365	29.515623
370.089687	21148.019587	29.520640
370.485550	21169.057441	29.525658
370.603748	21194.342590	29.530676
371.531189	21204.834110	29.535693
371.524627	21238.497023	29.540711
371.698378	21269.139564	29.545728
371.596617	21286.212851	29.550746
371.934565	21331.059622	29.555764
372.360310	21357.987398	29.560781
372.316769	21388.527319	29.565799
372.600291	21438.781403	29.570816
372.854760	21482.696449	29.575834
373.156111	21518.407429	29.580852
373.912472	21555.518965	29.585869
373.844230	21593.108915	29.590887
374.523580	21632.758973	29.595904
375.163605	21688.032985	29.600922
375.312956	21719.039833	29.605940
375.993369	21753.731723	29.610957
376.436972	21794.228309	29.615975
376.957684	21834.601894	29.620992
377.311547	21864.145276	29.626010
377.293611	21907.368598	29.631028
377.989802	21939.272455	29.636045
378.549982	21973.413941	29.641063
379.217392	22016.156983	29.646080
379.289754	22045.190651	29.651098
379.634736	22082.283023	29.656116
380.097682	22106.117310	29.661133
380.343504	22150.842750	29.666151
380.596104	22195.051640	29.671168
381.298822	22217.407036	29.676186
381.359713	22253.430479	29.681204
381.983329	22293.479153	29.686221
382.510585	22324.606002	29.691239
382.908522	22357.097550	29.696256
383.680491	22392.694808	29.701274
383.754417	22419.043875	29.706292
384.457138	22439.655821	29.711309
384.576654	22477.191503	29.716327
384.670329	22511.349658	29.721344
385.310195	22539.107955	29.726362
385.497035	22578.401727	29.731380
386.181958	22608.885014	29.736397
386.390333	22652.804426	29.741415
386.492992	22681.827881	29.746432
386.701200	22715.289570	29.751450
387.133603	22756.171873	29.756468
387.380086	22791.440545	29.761485
387.754507	22838.796934	29.766503
388.057777	22890.512086	29.771520
388.481069	22928.897293	29.776538
388.448311	22969.156911	29.781556
389.187032	23023.834063	29.786573
389.777842	23066.787939	29.791591
390.057795	23098.676041	29.796608
390.708037	23147.200205	29.801626
391.400093	23183.859263	29.806644
391.909577	23214.300100	29.811661
392.030658	23253.470711	29.816679
392.394059	23286.682427	29.821696
392.924193	23312.702101	29.826714
393.718581	23356.616412	29.831732
393.921422	23374.081398	29.836749
394.080783	23399.065061	29.841767
394.154026	23432.213048	29.846784
394.649806	23457.368271	29.851802
394.760206	23506.490351	29.856820
395.222989	23532.237678	29.861837
395.771282	23573.449698	29.866855
395.910697	23624.180324	29.871872
396.917789	23635.248348	29.876890
397.163806	23669.967073	29.881908
397.666964	23715.297461	29.886925
398.258866	23735.058940	29.891943
397.774411	23771.834788	29.896960
398.684768	23811.005602	29.901978
398.817642	23853.903103	29.906996
399.073932	23888.251617	29.912013
399.895098	23922.659834	29.917031
400.246310	23958.058703	29.922048
400.774297	23985.930896	29.927066
401.020226	24031.506450	29.932084
401.396215	24062.306721	29.937101
401.990914	24097.198933	29.942119
402.036251	24150.729695	29.947136
402.515229	24174.516957	29.952154
403.203376	24213.977698	29.957172
403.477246	24250.003326	29.962189
404.399112	24291.133308	29.967207
404.468220	24330.715502	29.972224
404.896948	24367.009082	29.977242
405.171338	24408.648393	29.982260
405.760151	24447.042817	29.987277
406.261114	24482.629337	29.992295
406.175604	24511.031056	29.997312
406.509633	24546.101282	30.002330
406.743679	24592.265305	30.007348
407.589682	24624.600474	30.012365
408.171331	24677.063513	30.017383
408.250316	24704.720921	30.022400
408.608823	24739.809580	30.027418
409.174376	24791.559744	30.032436
409.753167	24832.850210	30.037453
410.081123	24874.415585	30.042471
410.048792	24904.272495	30.047488
410.514104	24957.756921	30.052506
410.952539	25017.586535	30.057524
411.535558	25048.642963	30.062541
412.058140	25094.036902	30.067559
412.348686	25139.041958	30.072576
412.858350	25169.472089	30.077594
413.230286	25215.890980	30.082612
413.672339	25255.858400	30.087629
414.234458	25293.331937	30.092647
414.682540	25339.199288	30.097664
415.205807	25375.736440	30.102682
415.274256	25426.402168	30.107700
415.505912	25456.859814	30.112717
416.150151	25492.410589	30.117735
416.851333	25548.032465	30.122752
417.220603	25578.037097	30.127770
417.681556	25616.731246	30.132788
418.285904	25660.444804	30.137805
418.612249	25700.801382	30.142823
418.563043	25737.034910	30.147840
419.271734	25764.023898	30.152858
419.589149	25803.041797	30.157876
419.707152	25853.790493	30.162893
420.414611	25883.613642	30.167911
421.127755	25931.375292	30.172928
421.685181	25949.771526	30.177946
422.448296	25976.999443	30.182964
422.704623	26009.593929	30.187981
423.000589	26036.183169	30.192999
423.117553	26056.525707	30.198016
423.661089	26097.096504	30.203034
424.005628	26131.972715	30.208052
424.251679	26156.952417	30.213069
425.017120	26192.989263	30.218087
425.049060	26229.093733	30.223104
425.452883	26260.188280	30.228122
425.914055	26309.301504	30.233140
426.390859	26348.325859	30.238157
426.593901	26381.702581	30.243175
426.674229	26428.453643	30.248192
427.213693	26464.818558	30.253210
427.255245	26514.187771	30.258228
427.145528	26567.578256	30.263245
428.177973	26616.809314	30.268263
428.856581	26667.054637	30.273280
429.408633	26712.504784	30.278298
429.853764	26750.437679	30.283316
430.499349	26807.867496	30.288333
430.860711	26838.068044	30.293351
431.604632	26880.209865	30.298368
432.191799	26929.565842	30.303386
432.367865	26970.562131	30.308404
432.810676	26992.031584	30.313421
433.407226	27036.453312	30.318439
434.041207	27091.656044	30.323456
434.462620	27118.844450	30.328474
434.837567	27162.221246	30.333492
434.927605	27199.226547	30.338509
435.491433	27241.421083	30.343527
435.778956	27298.271397	30.348544
435.955241	27327.427812	30.353562
436.565108	27376.320817	30.358580
436.717707	27432.730200	30.363597
437.285535	27465.036279	30.368615
437.803221	27522.458071	30.373632
437.843915	27582.570529	30.378650
438.394387	27622.147061	30.383668
438.706124	27673.506284	30.388685
439.243387	27719.346354	30.393703
439.667617	27781.313922	30.398720
440.067928	27819.546771	30.403738
440.517856	27896.158845	30.408756
440.896995	27944.243079	30.413773
441.609971	27992.079892	30.418791
441.637591	28045.774008	30.423808
442.729083	28089.971604	30.428826
443.531878	28136.721520	30.433844
443.789674	28184.738148	30.438861
444.522721	28225.055561	30.443879
444.667061	28263.763820	30.448896
445.047681	28314.097878	30.453914
445.694396	28343.042666	30.458932
446.257658	28387.113784	30.463949
446.866337	28435.148853	30.468967
446.903627	28481.710718	30.473984
447.094289	28539.006960	30.479002
448.167504	28569.528265	30.484020
448.350127	28607.338278	30.489037
449.028662	28651.268008	30.494055
449.528730	28680.423697	30.499072
450.957468	28708.599579	30.504090
451.357521	28719.116677	30.509108
451.565883	28754.881857	30.514125
451.943394	28773.645213	30.519143
451.974973	28804.872093	30.524160
452.204479	28822.357170	30.529178
453.107343	28863.433478	30.534196
452.894135	28899.265438	30.539213
453.346557	28929.451457	30.544231
453.497898	28982.998714	30.549248
453.750030	29018.189404	30.554266
454.205800	29052.744024	30.559284
454.241013	29112.695518	30.564301
454.484222	29151.010892	30.569319
454.927861	29214.507166	30.574336
455.379402	29272.109735	30.579354
456.133789	29321.602664	30.584372
456.136707	29386.979910	30.589389
456.920287	29447.111777	30.594407
456.993921	29500.995230	30.599424
457.373439	29567.922926	30.604442
458.252866	29615.922857	30.609460
458.718317	29674.218470	30.614477
459.128392	29732.924058	30.619495
459.699461	29773.877521	30.624512
460.096401	29834.412137	30.629530
461.204949	29896.627558	30.634548
461.447080	29948.910406	30.639565
461.993693	29993.180794	30.644583
462.701068	30050.128527	30.649600
463.257223	30105.700755	30.654618
463.849201	30148.588611	30.659636
463.947670	30201.003206	30.664653
464.289733	30253.844615	30.669671
464.772462	30297.826634	30.674688
465.369405	30347.916341	30.679706
465.763551	30401.191252	30.684724
465.931437	30452.724434	30.689741
466.557151	30498.260705	30.694759
467.090896	30560.134937	30.699776
467.601667	30612.671948	30.704794
468.395078	30652.716885	30.709812
469.023893	30713.724173	30.714829
469.474726	30750.548112	30.719847
470.140437	30792.292807	30.724864
470.439846	30844.196613	30.729882
471.393014	30889.515768	30.734900
471.688116	30930.833017	30.739917
471.893825	30971.941138	30.744935
472.333140	31020.629679	30.749952
472.522013	31079.250146	30.754970
473.455321	31122.046159	30.759988
473.873696	31170.315827	30.765005
474.162572	31213.874721	30.770023
474.551531	31261.285066	30.775040
474.914003	31308.195134	30.780058
475.116164	31367.164561	30.785076
475.315854	31419.320006	30.790093
476.372232	31469.078339	30.795111
477.179905	31502.137900	30.800128
477.452278	31558.392611	30.805146
478.105650	31592.487407	30.810164
478.339242	31651.673445	30.815181
478.942158	31701.431622	30.820199
479.364916	31751.080881	30.825216
479.678005	31813.002303	30.830234
480.295231	31853.883615	30.835252
480.268004	31920.152400	30.840269
480.660763	31968.548388	30.845287
481.290913	32017.690894	30.850304
481.095556	32082.098210	30.855322
481.881623	32125.693980	30.860340
482.220581	32184.902270	30.865357
482.604436	32239.597933	30.870375
483.492990	32294.620559	30.875392
483.728853	32364.456948	30.880410
484.498002	32410.829528	30.885428
485.167698	32465.510230	30.890445
485.598952	32512.232314	30.895463
486.267898	32566.616875	30.900480
486.489932	32628.297489	30.905498
486.976039	32663.267567	30.910516
487.506244	32721.174556	30.915533
487.837930	32773.182855	30.920551
488.848582	32823.716131	30.925568
488.956199	32874.458661	30.930586
489.551961	32931.920102	30.935604
490.037582	32988.118919	30.940621
490.566775	33049.336941	30.945639
491.690906	33091.626655	30.950656
491.991117	33137.901919	30.955674
492.490095	33181.074445	30.960692
492.817611	33234.936906	30.965709
493.198880	33283.672860	30.970727
493.901966	33334.056469	30.975744
494.343991	33383.694530	30.980762
494.872423	33427.209871	30.985780
495.053543	33477.465547	30.990797
495.414940	33533.279589	30.995815
495.993657	33589.404992	31.000832
496.272714	33661.025269	31.005850
497.152664	33712.882669	31.010868
497.435352	33775.005321	31.015885
497.854190	33837.392838	31.020903
499.145834	33875.864056	31.025920
499.841348	33915.522418	31.030938
500.639360	33967.719101	31.035956
501.271496	34000.695612	31.040973
501.314110	34047.545905	31.045991
501.976280	34090.539084	31.051008
502.133553	34131.022037	31.056026
502.987464	34176.460733	31.061044
503.243324	34241.650186	31.066061
503.623135	34290.073611	31.071079
504.290597	34344.104176	31.076096
504.202234	34392.766138	31.081114
504.592713	34440.550815	31.086132
505.094351	34509.354654	31.091149
505.288142	34567.632491	31.096167
505.861658	34618.735361	31.101184
506.604745	34689.077752	31.106202
507.146281	34744.480882	31.111220
507.408229	34801.097902	31.116237
507.898898	34862.214954	31.121255
509.139164	34904.253165	31.126272
509.836185	34954.973717	31.131290
510.797684	34994.590561	31.136308
511.516869	35031.581081	31.141325
511.888746	35089.017080	31.146343
512.502708	35120.796410	31.151360
512.378273	35174.026252	31.156378
513.117834	35217.757250	31.161396
513.351648	35260.054055	31.166413
513.600304	35310.104959	31.171431
514.194411	35357.416682	31.176448
514.809793	35410.900550	31.181466
515.212407	35469.301470	31.186484
515.779198	35516.567637	31.191501
516.065383	35568.806232	31.196519
516.712171	35619.038383	31.201536
516.953042	35666.172596	31.206554
517.103183	35717.967061	31.211572
517.736472	35777.138738	31.216589
518.109826	35835.561467	31.221607
518.868253	35875.870199	31.226624
519.504318	35936.127503	31.231642
520.178935	35979.419832	31.236660
520.766621	36045.138568	31.241677
520.974098	36094.715646	31.246695
521.550182	36142.335377	31.251712
521.555963	36210.123172	31.256730
521.967944	36260.440090	31.261748
522.855360	36329.045221	31.266765
523.092323	36395.397524	31.271783
523.513845	36449.345707	31.276800
523.846225	36530.508684	31.281818
524.407446	36599.863009	31.286836
525.067204	36658.181155	31.291853
525.387771	36738.204611	31.296871
526.390242	36793.815681	31.301888
526.543871	36862.903824	31.306906
527.213049	36927.125920	31.311924
528.142927	37001.050580	31.316941
528.811877	37059.548399	31.321959
529.830182	37115.523937	31.326976
530.353123	37172.502999	31.331994
530.982141	37214.063775	31.337012
531.537326	37282.042590	31.342029
531.947254	37335.190585	31.347047
532.508911	37379.287631	31.352064
532.764836	37438.858499	31.357082
533.329455	37494.152720	31.362100
533.641406	37557.814345	31.367117
533.885418	37629.677241	31.372135
534.906675	37678.991727	31.377152
535.779035	37745.875266	31.382170
536.467945	37798.505146	31.387188
537.102902	37838.945993	31.392205
536.997968	37903.097447	31.397223
537.859380	37956.980654	31.402240
538.733015	38006.115275	31.407258
539.667446	38051.799865	31.412276
540.321133	38087.567185	31.417293
540.385746	38138.719975	31.422311
541.050738	38206.494776	31.427328
541.579329	38245.366584	31.432346
541.635032	38290.016531	31.437364
542.591201	38353.842829	31.442381
542.636258	38416.065026	31.447399
543.113812	38467.298879	31.452416
543.400981	38526.129634	31.457434
543.985652	38589.992877	31.462452
544.356084	38652.461980	31.467469
545.105169	38716.399511	31.472487
545.687769	38786.449927	31.477504
545.826651	38863.514425	31.482522
546.362927	38927.257445	31.487540
546.994978	38991.527744	31.492557
547.059852	39071.739495	31.497575
547.642954	39138.480278	31.502592
548.344411	39211.549032	31.507610
548.339686	39289.825818	31.512628
549.200492	39364.248168	31.517645
549.469236	39442.852887	31.522663
550.573225	39523.172759	31.527680
550.873921	39594.661642	31.532698
551.194425	39675.190499	31.537716
552.249645	39746.356505	31.542733
552.316306	39818.263684	31.547751
552.970110	39875.381152	31.552768
553.942927	39958.423329	31.557786
554.113295	40024.288611	31.562804
554.834921	40084.608769	31.567821
554.835394	40170.697488	31.572839
555.515047	40238.922516	31.577856
556.229197	40331.386949	31.582874
556.487880	40394.527570	31.587892
557.713333	40460.062335	31.592909
558.243995	40536.857718	31.597927
559.153016	40592.249705	31.602944
559.516821	40673.782747	31.607962
560.224676	40743.962054	31.612980
561.009011	40797.664412	31.617997
561.340951	40876.586839	31.623015
561.793441	40940.757942	31.628032
562.783982	41003.432565	31.633050
563.162863	41071.419973	31.638068
563.927025	41122.096280	31.643085
564.311314	41210.064654	31.648103
564.893278	41269.508999	31.653120
565.525478	41341.193024	31.658138
565.997119	41406.937763	31.663156
566.695003	41473.065208	31.668173
567.142579	41549.828056	31.673191
567.536571	41620.226708	31.678208
568.450850	41684.860783	31.683226
568.938369	41760.175299	31.688244
569.738360	41816.633876	31.693261
569.742431	41896.637622	31.698279
570.254884	41953.548173	31.703296
571.067431	42020.283688	31.708314
571.572490	42110.493512	31.713332
572.433839	42182.370261	31.718349
572.352193	42255.233278	31.723367
573.168501	42315.968163	31.728384
573.935566	42404.418846	31.733402
574.691403	42483.795885	31.738420
575.420211	42546.667380	31.743437
575.802306	42629.203646	31.748455
576.458914	42684.624705	31.753472
577.102030	42753.288143	31.758490
577.787491	42822.626734	31.763508
578.215939	42887.285294	31.768525
578.691381	42962.859274	31.773543
579.569013	43027.573571	31.778560
580.080673	43097.901609	31.783578
580.437592	43172.179572	31.788596
581.685103	43235.150848	31.793613
582.186841	43301.793959	31.798631
582.975609	43359.351434	31.803648
583.167726	43426.096642	31.808666
583.786263	43493.466205	31.813684
584.279069	43549.321010	31.818701
584.730787	43627.253604	31.823719
585.536437	43697.671118	31.828736
586.360137	43758.194848	31.833754
586.735277	43822.499261	31.838772
587.403761	43887.371079	31.843789
588.019688	43950.076567	31.848807
588.215103	44010.714361	31.853824
588.948293	44081.770407	31.858842
589.155148	44150.211155	31.863860
589.824982	44223.778653	31.868877
590.838212	44300.371106	31.873895
591.161082	44367.688490	31.878912
591.599098	44432.796021	31.883930
591.875883	44500.143596	31.888948
592.643849	44552.154721	31.893965
593.090333	44639.336692	31.898983
593.317808	44710.162942	31.904000
594.193581	44766.131802	31.909018
594.474546	44847.646441	31.914036
594.950388	44917.731551	31.919053
595.480556	45000.920091	31.924071
595.935716	45090.180219	31.929088
596.682142	45167.972717	31.934106
597.169951	45255.318076	31.939124
598.488254	45318.650982	31.944141
599.110022	45390.826017	31.949159
599.699187	45468.696258	31.954176
600.846111	45531.253068	31.959194
601.104018	45609.140716	31.964212
601.956230	45676.700605	31.969229
602.515855	45750.036578	31.974247
602.757028	45825.266203	31.979264
603.601296	45889.667607	31.984282
604.218500	45966.385987	31.989300
604.848589	46026.469136	31.994317
605.468311	46092.657548	31.999335
605.881498	46187.123853	32.004352
606.387236	46255.033539	32.009370
606.798092	46334.304017	32.014388
607.689503	46425.130883	32.019405
608.167243	46495.606804	32.024423
608.439683	46574.070725	32.029440
609.015865	46668.787236	32.034458
609.768841	46740.595310	32.039476
610.722903	46816.415302	32.044493
611.281959	46905.073287	32.049511
611.492954	46980.100960	32.054528
612.483591	47068.887366	32.059546
613.104775	47145.395184	32.064564
614.062818	47226.903066	32.069581
614.488025	47309.440285	32.074599
614.896104	47394.873120	32.079616
615.963609	47454.645450	32.084634
616.392751	47540.675426	32.089652
617.483616	47614.382484	32.094669
617.997098	47686.789475	32.099687
618.077641	47773.279114	32.104704
619.087469	47840.896537	32.109722
619.661419	47909.277740	32.114740
620.137664	47992.643161	32.119757
620.686051	48084.071495	32.124775
621.198250	48149.473340	32.129792
621.872686	48229.892425	32.134810
622.056919	48312.031722	32.139828
622.644288	48399.485753	32.144845
623.413298	48492.095385	32.149863
623.967625	48580.146225	32.154880
624.899067	48653.384718	32.159898
625.562441	48762.118320	32.164916
626.526878	48827.492023	32.169933
627.060873	48900.250790	32.174951
627.457440	48987.328510	32.179968
628.297590	49060.416280	32.184986
629.043372	49146.470721	32.190004
629.468579	49228.754185	32.195021
629.833694	49309.696308	32.200039
630.098281	49387.955284	32.205056
630.724016	49476.734294	32.210074
631.262146	49574.155936	32.215092
631.767573	49655.638484	32.220109
632.734591	49742.619125	32.225127
632.857376	49836.381029	32.230144
633.749295	49922.187454	32.235162
634.375384	50000.045003	32.240180
635.074294	50099.198675	32.245197
635.906436	50174.714318	32.250215
636.263445	50269.725022	32.255232
636.792554	50346.096717	32.260250
637.338217	50435.821907	32.265268
637.961090	50535.549394	32.270285
638.509561	50619.744986	32.275303
639.080394	50717.782900	32.280320
639.678595	50815.030394	32.285338
640.450780	50917.053352	32.290356
641.213585	50998.066425	32.295373
642.394271	51098.165820	32.300391
643.454110	51177.365113	32.305408
644.037784	51249.249766	32.310426
645.032008	51330.516587	32.315444
645.608358	51404.380141	32.320461
646.981805	51462.927006	32.325479
647.410106	51551.811406	32.330496
648.293097	51623.730144	32.335514
648.795111	51693.175888	32.340532
649.256276	51771.671114	32.345549
649.695456	51835.436318	32.350567
650.116329	51920.855717	32.355584
650.584972	51999.878092	32.360602
651.320401	52081.768818	32.365620
651.903911	52161.474060	32.370637
652.574165	52240.271457	32.375655
653.124401	52322.515953	32.380672
654.255691	52397.501362	32.385690
654.606695	52486.949254	32.390708
655.240256	52559.863387	32.395725
656.088732	52645.869186	32.400743
656.488768	52732.138939	32.405760
657.230885	52825.080330	32.410778
657.624797	52902.697379	32.415796
658.218997	53006.441148	32.420813
659.148152	53077.533281	32.425831
659.476758	53168.744203	32.430848
660.357077	53264.033842	32.435866
660.527355	53356.352046	32.440884
661.110733	53448.324503	32.445901
662.239727	53532.323213	32.450919
662.659227	53640.218139	32.455936
663.329885	53732.891393	32.460954
664.247206	53826.604638	32.465972
664.458519	53915.374620	32.470989
664.993877	54025.994339	32.476007
665.800765	54132.172821	32.481024
666.196637	54220.629421	32.486042
667.387420	54312.448787	32.491060
667.972929	54425.576900	32.496077
668.606161	54506.603942	32.501095
669.212919	54599.557209	32.506112
670.271566	54695.096058	32.511130
670.960041	54785.970813	32.516148
671.193208	54881.526861	32.521165
672.146612	54975.258614	32.526183
672.716766	55076.926167	32.531200
673.328501	55175.497928	32.536218
673.974675	55267.222182	32.541236
674.396718	55368.915708	32.546253
675.146575	55467.883113	32.551271
675.580197	55583.273243	32.556288
676.138362	55673.655554	32.561306
676.743222	55772.414669	32.566324
677.367977	55880.117455	32.571341
678.214948	55967.471266	32.576359
679.033066	56072.281048	32.581376
679.234675	56166.180550	32.586394
680.000570	56260.587544	32.591412
680.352257	56373.765495	32.596429
681.458635	56475.749774	32.601447
681.938450	56588.452878	32.606464
682.460369	56695.829591	32.611482
683.621671	56795.828799	32.616500
684.164510	56896.505628	32.621517
685.173730	56993.409639	32.626535
686.249891	57097.499853	32.631552
686.795959	57190.576477	32.636570
688.125897	57284.838349	32.641588
688.317723	57384.292956	32.646605
689.510712	57469.024596	32.651623
690.241553	57563.601566	32.656640
690.548022	57654.028184	32.661658
691.252111	57748.781058	32.666676
691.510001	57853.067241	32.671693
692.206022	57958.128333	32.676711
692.745566	58059.361342	32.681728
693.855447	58160.178417	32.686746
695.154258	58250.273258	32.691764
695.854681	58350.293230	32.696781
696.808858	58432.995820	32.701799
697.391153	58529.232199	32.706816
697.798547	58617.826665	32.711834
698.512471	58721.277482	32.716852
698.679750	58813.255234	32.721869
699.752795	58899.143888	32.726887
700.193116	59010.268521	32.731904
700.424403	59116.442479	32.736922
701.254161	59222.543443	32.741940
701.603008	59330.177810	32.746957
702.599071	59436.941242	32.751975
703.505680	59552.213138	32.756992
704.458080	59642.169253	32.762010
705.535563	59740.939563	32.767028
705.954558	59846.915768	32.772045
706.869328	59936.076855	32.777063
707.505794	60044.173106	32.782080
707.964051	60154.271045	32.787098
708.821960	60255.911275	32.792116
709.219948	60362.652008	32.797133
710.093044	60471.570936	32.802151
710.446444	60582.434241	32.807168
711.370979	60680.071616	32.812186
712.103964	60790.949218	32.817204
712.632983	60911.125814	32.822221
713.154047	61010.676775	32.827239
713.858470	61126.553537	32.832256
714.518491	61254.439636	32.837274
715.258781	61357.798555	32.842292
715.717702	61484.392147	32.847309
716.768519	61600.296578	32.852327
717.417368	61719.017238	32.857344
718.101760	61829.068000	32.862362
719.222771	61935.893557	32.867380
719.915887	62047.157508	32.872397
720.663616	62147.776317	32.877415
721.449029	62266.446026	32.882432
721.812292	62380.995866	32.887450
722.834026	62483.593544	32.892468
723.089825	62600.917977	32.897485
724.331912	62697.065298	32.902503
725.199388	62794.286185	32.907520
725.743564	62900.706446	32.912538
726.931323	62990.758684	32.917556
727.016449	63094.797143	32.922573
728.103153	63203.872445	32.927591
728.653614	63306.874434	32.932608
728.947193	63403.826410	32.937626
729.908924	63512.412037	32.942644
730.808939	63627.834634	32.947661
731.159073	63726.586479	32.952679
731.800015	63840.561398	32.957696
732.283164	63953.121899	32.962714
733.214699	64067.435652	32.967732
733.588400	64204.514630	32.972749
734.216484	64306.263638	32.977767
735.176756	64428.968639	32.982784
735.803994	64562.613864	32.987802
736.842574	64676.123221	32.992820
737.610899	64794.216251	32.997837
738.075869	64922.814913	33.002855
738.772899	65040.143648	33.007872
739.404425	65158.343527	33.012890
740.515791	65289.315573	33.017908
741.384557	65407.958105	33.022925
742.692929	65516.705673	33.027943
743.652635	65631.377439	33.032960
744.498906	65733.015282	33.037978
745.516331	65849.985968	33.042996
746.024416	65954.000637	33.048013
746.640458	66069.749307	33.053031
747.739678	66182.991438	33.058048
748.268096	66288.098017	33.063066
748.636549	66388.806560	33.068084
749.213227	66519.027612	33.073101
750.087557	66626.272320	33.078119
750.454490	66756.693854	33.083136
751.034985	66882.744352	33.088154
751.984597	67002.217097	33.093172
752.296742	67132.972433	33.098189
753.087738	67273.245810	33.103207
754.002311	67393.105881	33.108224
754.491812	67517.632743	33.113242
755.784912	67646.326458	33.118260
756.336559	67777.659491	33.123277
757.398722	67895.234856	33.128295
758.102441	68010.423500	33.133312
759.036439	68145.128488	33.138330
759.462152	68269.537593	33.143348
760.493413	68398.873438	33.148365
761.151750	68531.723502	33.153383
761.821439	68649.140311	33.158400
763.304442	68759.266831	33.163418
764.979806	68854.403954	33.168436
766.005248	68968.413063	33.173453
766.461438	69070.397104	33.178471
767.140235	69176.454338	33.183488
767.510111	69290.630345	33.188506
768.396670	69402.907145	33.193524
768.873307	69513.026767	33.198541
769.107601	69621.732834	33.203559
770.042062	69742.058238	33.208576
770.883816	69875.449177	33.213594
771.565846	69994.749207	33.218612
771.800517	70125.649749	33.223629
772.355298	70252.812182	33.228647
773.710148	70360.135712	33.233664
774.127739	70506.859160	33.238682
774.945129	70636.813072	33.243700
775.398245	70747.025183	33.248717
776.092606	70874.440164	33.253735
777.072728	70991.363476	33.258752
777.759248	71104.706613	33.263770
778.452748	71223.828290	33.268788
779.141375	71355.786908	33.273805
780.316327	71467.957462	33.278823
781.009966	71589.129784	33.283840
781.886595	71722.988131	33.288858
782.761809	71845.213155	33.293876
783.505317	71975.952518	33.298893
783.995643	72107.082258	33.303911
784.973955	72214.964193	33.308928
785.066699	72366.047478	33.313946
785.855720	72494.360705	33.318964
786.819523	72619.598022	33.323981
787.436025	72762.484857	33.328999
788.389876	72898.329634	33.334016
788.957321	73042.307720	33.339034
789.749161	73188.260567	33.344052
790.795050	73318.913908	33.349069
791.869888	73463.177783	33.354087
792.364201	73610.592761	33.359104
792.933759	73753.399063	33.364122
794.292118	73892.952177	33.369140
795.271878	74020.863579	33.374157
795.765118	74160.947021	33.379175
796.439367	74295.904529	33.384192
797.319029	74450.394794	33.389210
798.023539	74588.561618	33.394228
798.934626	74726.069145	33.399245
799.778120	74865.574415	33.404263
800.499247	75010.242170	33.409280
801.428374	75153.219650	33.414298
802.121295	75294.390450	33.419316
803.024267	75434.774913	33.424333
803.733613	75581.446816	33.429351
804.930275	75732.029790	33.434368
805.673838	75866.467008	33.439386
806.638421	76001.298605	33.444404
807.614516	76146.108865	33.449421
808.229837	76283.712996	33.454439
809.206574	76430.934605	33.459456
810.365119	76569.443756	33.464474
811.010618	76688.673024	33.469492
812.394424	76829.113522	33.474509
813.163035	76966.456291	33.479527
814.405302	77064.566329	33.484544
815.020471	77184.650786	33.489562
815.981446	77313.659768	33.494580
816.673027	77435.567118	33.499597
817.193717	77566.800669	33.504615
818.189755	77690.879126	33.509632
818.845676	77818.739733	33.514650
819.683902	77944.920202	33.519668
820.207201	78072.538533	33.524685
820.746266	78221.963204	33.529703
821.860167	78347.771554	33.534720
822.356878	78479.937919	33.539738
823.171831	78613.197346	33.544756
824.012058	78739.831085	33.549773
824.595847	78890.290176	33.554791
825.426122	79033.859477	33.559808
826.292835	79178.018253	33.564826
826.657401	79327.985187	33.569844
827.679694	79465.206684	33.574861
828.346063	79607.604950	33.579879
829.273310	79759.872831	33.584896
829.575535	79907.153032	33.589914
830.579050	80041.673914	33.594932
831.348852	80188.182963	33.599949
832.164611	80333.363354	33.604967
833.040872	80459.671976	33.609984
833.972832	80604.044242	33.615002
834.889536	80742.600399	33.620020
835.978121	80888.732453	33.625037
836.639627	81043.608493	33.630055
837.413379	81163.979204	33.635072
838.189645	81313.897765	33.640090
839.193503	81468.511445	33.645108
839.631578	81610.251619	33.650125
840.429957	81772.138076	33.655143
841.392347	81908.074937	33.660160
841.963081	82063.997766	33.665178
842.936719	82208.803592	33.670196
844.362286	82366.105594	33.675213
844.911466	82522.718352	33.680231
846.193419	82659.220586	33.685248
847.014261	82812.462936	33.690266
847.547975	82971.599160	33.695284
848.411170	83113.354445	33.700301
849.359366	83263.662396	33.705319
850.286771	83414.613732	33.710336
851.114213	83573.686680	33.715354
851.962818	83726.114484	33.720372
853.060699	83869.898137	33.725389
853.790718	84036.461960	33.730407
854.654717	84189.643166	33.735424
855.755826	84333.055928	33.740442
856.388438	84487.517344	33.745460
857.479292	84642.479863	33.750477
858.052009	84791.411034	33.755495
859.432429	84934.756129	33.760512
860.348638	85090.503391	33.765530
861.147511	85222.393547	33.770548
862.526985	85368.177334	33.775565
862.863891	85528.300180	33.780583
863.891775	85665.691122	33.785600
864.720409	85813.776787	33.790618
865.532741	85965.080232	33.795636
866.500335	86108.456495	33.800653
866.929010	86263.374733	33.805671
867.845516	86427.723200	33.810688
868.602554	86583.133490	33.815706
869.233145	86739.945041	33.820724
870.501551	86893.602575	33.825741
871.104712	87054.223481	33.830759
872.127186	87212.808440	33.835776
872.930029	87374.626096	33.840794
873.571646	87522.861094	33.845812
874.398366	87687.321856	33.850829
875.391158	87869.106535	33.855847
876.206825	88020.903681	33.860864
876.670762	88184.105362	33.865882
877.528555	88359.329047	33.870900
878.717703	88510.257747	33.875917
879.451708	88697.368906	33.880935
880.138526	88868.176178	33.885952
881.144606	89020.346993	33.890970
882.389552	89190.621497	33.895988
883.493676	89355.041800	33.901005
884.491568	89521.898087	33.906023
885.258020	89689.002592	33.911040
885.789450	89851.913582	33.916058
886.612354	90010.398492	33.921076
887.465506	90178.390728	33.926093
888.157220	90335.266796	33.931111
888.989204	90506.397318	33.936128
889.716768	90664.459354	33.941146
890.400885	90824.681253	33.946164
891.223350	90987.241880	33.951181
891.876362	91170.386386	33.956199
893.289503	91339.211975	33.961216
894.094230	91499.000805	33.966234
894.723973	91680.615226	33.971252
895.575256	91850.714310	33.976269
896.052768	92019.357431	33.981287
897.096157	92211.242297	33.986304
897.918670	92391.513894	33.991322
898.755961	92582.682629	33.996340
899.832843	92762.345409	34.001357
900.836193	92961.046396	34.006375
901.422020	93126.723781	34.011392
902.856166	93315.192240	34.016410
903.370197	93513.155785	34.021428
904.766356	93686.867706	34.026445
905.542721	93875.695968	34.031463
906.654730	94057.311946	34.036480
907.437973	94239.103819	34.041498
908.127699	94433.950855	34.046516
908.993469	94614.466043	34.051533
910.264402	94804.840170	34.056551
911.395343	94983.333203	34.061568
912.895210	95166.690974	34.066586
913.856601	95346.657779	34.071604
914.914076	95531.755997	34.076621
916.037567	95696.887377	34.081639
916.716722	95874.372802	34.086656
917.841663	96044.626990	34.091674
918.632281	96215.981967	34.096692
919.902222	96377.346518	34.101709
920.565729	96548.813414	34.106727
921.432370	96724.995382	34.111744
922.518980	96880.633291	34.116762
923.196482	97067.970629	34.121780
924.178716	97249.910196	34.126797
925.112168	97426.845733	34.131815
925.552073	97610.365053	34.136832
926.838156	97803.912269	34.141850
927.551083	97980.603302	34.146868
928.367843	98149.409932	34.151885
929.373191	98340.981992	34.156903
929.929407	98528.692196	34.161920
931.433772	98710.657521	34.166938
932.294069	98902.251503	34.171956
933.344180	99073.849231	34.176973
934.448514	99257.315268	34.181991
935.146932	99451.877546	34.187008
936.107646	99633.420222	34.192026
937.105726	99811.862338	34.197044
938.027737	99990.539852	34.202061
938.534861	100188.595978	34.207079
939.637839	100380.515677	34.212096
940.648616	100557.726460	34.217114
941.602284	100738.771782	34.222132
942.679359	100931.307702	34.227149
943.848665	101128.749048	34.232167
944.354812	101295.431207	34.237184
945.813076	101473.828058	34.242202
946.831326	101655.103501	34.247220
947.702397	101841.507467	34.252237
948.728824	102021.486272	34.257255
949.605297	102197.236488	34.262272
950.578108	102367.178853	34.267290
951.304458	102561.665397	34.272308
952.176635	102720.363229	34.277325
953.301807	102888.682053	34.282343
953.972713	103072.291541	34.287360
954.991318	103231.056994	34.292378
955.865073	103408.899030	34.297396
956.993684	103583.122854	34.302413
957.815657	103760.178079	34.307431
958.494560	103949.915208	34.312448
959.560725	104117.137419	34.317466
960.360469	104294.681184	34.322484
961.281827	104489.662950	34.327501
962.268168	104675.650512	34.332519
963.090111	104863.148218	34.337536
964.083423	105059.211468	34.342554
964.871760	105237.871655	34.347572
965.616103	105435.460531	34.352589
966.896910	105627.997956	34.357607
967.782879	105825.477748	34.362624
968.916247	106025.210444	34.367642
969.680684	106217.660156	34.372660
970.426902	106431.061542	34.377677
971.275150	106632.454335	34.382695
972.378081	106841.038225	34.387712
973.548143	107036.821130	34.392730
974.396276	107235.850215	34.397748
975.736030	107437.319987	34.402765
976.798625	107640.876148	34.407783
977.266464	107855.284896	34.412800
978.896257	108047.655743	34.417818
979.794001	108256.297330	34.422836
980.938468	108447.864616	34.427853
982.321939	108652.756102	34.432871
982.965840	108857.682603	34.437888
983.932269	109059.707606	34.442906
984.762600	109269.837488	34.447924
985.565579	109480.657501	34.452941
986.333539	109686.367822	34.457959
987.175704	109893.194764	34.462976
988.037360	110103.718653	34.467994
989.083076	110323.282983	34.473012
990.190484	110539.659609	34.478029
991.341572	110757.272088	34.483047
992.219562	110972.056050	34.488064
992.792392	111194.707549	34.493082
994.082316	111418.977861	34.498100
995.267017	111637.630547	34.503117
996.147953	111855.853787	34.508135
997.320720	112073.916589	34.513152
998.298333	112294.458155	34.518170
999.371402	112512.819602	34.523188
1000.141665	112731.853493	34.528205
1001.576109	112939.163219	34.533223
1002.528913	113159.943864	34.538240
1003.739886	113366.343625	34.543258
1004.888137	113582.484287	34.548276
1005.986351	113788.424442	34.553293
1007.506289	113996.614782	34.558311
1008.598460	114208.449760	34.563328
1009.589282	114398.665548	34.568346
1010.680284	114596.087108	34.573364
1011.588737	114806.234074	34.578381
1012.803517	114998.152583	34.583399
1014.091577	115196.229977	34.588416
1015.216042	115381.122234	34.593434
1016.503636	115565.811419	34.598452
1017.774371	115748.211527	34.603469
1018.508978	115931.702188	34.608487
1019.671882	116105.355449	34.613504
1020.453921	116280.960373	34.618522
1021.138590	116460.117196	34.623540
1022.189323	116651.668710	34.628557
1023.152248	116825.625491	34.633575
1024.259406	117009.720491	34.638592
1025.119876	117186.597732	34.643610
1025.586972	117374.322924	34.648628
1026.436612	117570.753690	34.653645
1027.679483	117764.282848	34.658663
1027.996727	117963.806983	34.663680
1029.074956	118155.351463	34.668698
1030.115785	118372.192980	34.673716
1030.804126	118589.284390	34.678733
1031.949150	118776.856235	34.683751
1032.727924	119002.944450	34.688768
1033.879460	119213.020739	34.693786
1035.063504	119439.514299	34.698804
1035.976211	119667.701630	34.703821
1037.040996	119871.360335	34.708839
1038.113461	120101.602738	34.713856
1039.381219	120310.717535	34.718874
1040.771348	120526.440618	34.723892
1041.096275	120751.705159	34.728909
1042.421672	120964.553159	34.733927
1043.378758	121179.997796	34.738944
1044.406040	121415.681439	34.743962
1045.757846	121628.859397	34.748980
1046.247105	121852.635423	34.753997
1047.814871	122087.893131	34.759015
1048.432511	122320.255662	34.764032
1049.331349	122549.443635	34.769050
1050.341751	122794.556431	34.774068
1051.410476	123022.516197	34.779085
1052.614116	123253.661534	34.784103
1053.149755	123505.384826	34.789120
1054.489647	123745.331482	34.794138
1055.719080	123987.047131	34.799156
1056.436244	124228.988713	34.804173
1058.110960	124457.708550	34.809191
1058.958707	124706.526443	34.814208
1059.911221	124951.552563	34.819226
1060.919195	125195.164821	34.824244
1062.282813	125430.824950	34.829261
1063.481636	125669.251563	34.834279
1064.281032	125910.458111	34.839296
1065.540821	126152.794566	34.844314
1066.685961	126400.829663	34.849332
1067.342673	126646.146537	34.854349
1068.553879	126886.190275	34.859367
1069.438785	127144.400783	34.864384
1070.627002	127390.079510	34.869402
1072.009834	127623.345488	34.874420
1072.942251	127871.022128	34.879437
1074.245252	128111.592682	34.884455
1075.289612	128352.423286	34.889472
1076.325969	128594.233037	34.894490
1077.698679	128840.108411	34.899508
1078.520972	129094.125050	34.904525
1079.283963	129333.463461	34.909543
1080.199069	129590.586860	34.914560
1081.282658	129832.588634	34.919578
1082.425240	130097.385089	34.924596
1083.358542	130355.234295	34.929613
1084.610370	130606.124997	34.934631
1085.723026	130868.372524	34.939648
1086.429374	131115.795565	34.944666
1087.608792	131362.584735	34.949684
1088.988407	131615.351092	34.954701
1090.806304	131830.691461	34.959719
1091.867323	132070.965008	34.964736
1093.166694	132292.732088	34.969754
1094.525197	132506.505022	34.974772
1095.142204	132750.533091	34.979789
1096.549243	132962.019368	34.984807
1097.793066	133198.075433	34.989824
1098.458137	133422.541089	34.994842
1099.287674	133648.274181	34.999860
1100.440742	133897.572037	35.004877
1101.550910	134120.181704	35.009895
1102.524549	134358.471329	35.014912
1104.058671	134592.803735	35.019930
1105.399859	134823.252499	35.024948
1106.042873	135071.160436	35.029965
1107.155087	135303.184349	35.034983
1108.392600	135554.965813	35.040000
1109.131003	135793.279489	35.045018
1110.244425	136032.344361	35.050036
1111.356267	136290.199416	35.055053
1112.411506	136532.003231	35.060071
1113.337753	136792.187538	35.065088
1114.391875	137036.670270	35.070106
1115.563741	137296.627859	35.075124
1116.110177	137562.535331	35.080141
1117.272771	137826.124550	35.085159
1118.341523	138085.268608	35.090176
1119.297513	138353.536376	35.095194
1121.027590	138627.662768	35.100212
1121.715471	138900.873097	35.105229
1122.987401	139166.001680	35.110247
1124.418437	139432.779698	35.115264
1125.230590	139707.586303	35.120282
1126.629474	139979.103195	35.125300
1127.507299	140254.981142	35.130317
1128.574840	140537.207662	35.135335
1129.693176	140811.313395	35.140352
1130.868477	141084.739932	35.145370
1132.469292	141352.696958	35.150388
1133.399824	141632.787001	35.155405
1134.830826	141899.939503	35.160423
1136.008074	142176.988187	35.165440
1137.090666	142444.785719	35.170458
1138.467229	142704.523047	35.175476
1139.379005	142983.054884	35.180493
1140.728598	143253.008278	35.185511
1142.173589	143523.899051	35.190528
1143.228247	143803.732653	35.195546
1144.179769	144065.148077	35.200564
1145.040267	144339.425930	35.205581
1146.536442	144618.457711	35.210599
1147.774180	144886.743014	35.215616
1149.019856	145153.139602	35.220634
1150.420933	145430.532335	35.225652
1151.112040	145704.886851	35.230669
1152.324829	145970.952651	35.235687
1153.334251	146245.309531	35.240704
1154.147326	146529.199295	35.245722
1155.575462	146793.549080	35.250740
1156.605678	147073.869200	35.255757
1157.557247	147368.534795	35.260775
1158.705896	147648.408679	35.265792
1159.418592	147930.208255	35.270810
1160.477729	148213.829777	35.275828
1161.881467	148504.321056	35.280845
1162.989964	148791.667486	35.285863
1163.954030	149088.196635	35.290880
1165.370111	149365.021251	35.295898
1166.427688	149639.028220	35.300916
1167.573106	149913.149563	35.305933
1168.830320	150173.506492	35.310951
1170.261281	150450.514401	35.315968
1171.328696	150727.749276	35.320986
1172.752379	151001.363512	35.326004
1173.534162	151279.994057	35.331021
1174.512035	151572.431621	35.336039
1175.930520	151845.215835	35.341056
1177.186318	152120.768491	35.346074
1179.017852	152389.429828	35.351092
1180.093192	152665.206520	35.356109
1181.724814	152939.155755	35.361127
1182.590851	153216.467690	35.366144
1183.451318	153503.434935	35.371162
1184.831581	153777.786873	35.376180
1185.792023	154052.654024	35.381197
1186.942626	154342.065755	35.386215
1188.091679	154632.152191	35.391232
1189.160738	154912.093933	35.396250
1190.532923	155195.196817	35.401268
1191.898713	155506.449619	35.406285
1192.709047	155779.882500	35.411303
1193.932373	156070.398760	35.416320
1194.870478	156373.065501	35.421338
1196.683031	156653.074682	35.426356
1197.781760	156945.736390	35.431373
1198.913731	157248.187625	35.436391
1200.070755	157538.446655	35.441408
1200.981168	157842.841788	35.446426
1202.631457	158136.968895	35.451444
1203.870572	158427.804420	35.456461
1205.347119	158736.895354	35.461479
1206.716978	159026.216776	35.466496
1207.514299	159321.559000	35.471514
1208.895191	159616.616785	35.476532
1209.968058	159915.710934	35.481549
1211.207532	160201.484916	35.486567
1212.650616	160502.615477	35.491584
1213.637695	160826.227269	35.496602
1214.650399	161107.731761	35.501620
1216.068469	161408.365692	35.506637
1217.285823	161728.140711	35.511655
1218.726911	162021.303023	35.516672
1219.638155	162325.363863	35.521690
1220.596047	162632.286430	35.526708
1222.295597	162930.119284	35.531725
1223.712960	163234.636087	35.536743
1225.170836	163534.568422	35.541760
1226.262851	163837.037270	35.546778
1227.285338	164139.507081	35.551796
1228.504473	164443.278764	35.556813
1229.411881	164741.483587	35.561831
1230.744447	165045.684921	35.566848
1231.698801	165366.533449	35.571866
1232.640502	165680.725471	35.576884
1233.921556	166002.146532	35.581901
1235.079079	166327.713921	35.586919
1236.494923	166633.651004	35.591936
1237.476901	166966.357400	35.596954
1238.596600	167273.692803	35.601972
1240.332912	167597.093338	35.606989
1241.527877	167926.295339	35.612007
1243.242669	168231.280733	35.617024
1244.102495	168556.368292	35.622042
1245.372880	168869.285600	35.627060
1246.747693	169175.945071	35.632077
1247.757423	169480.065723	35.637095
1249.157075	169786.141609	35.642112
1250.052919	170085.412670	35.647130
1251.679828	170375.898488	35.652148
1252.534058	170690.343762	35.657165
1253.608933	170998.270646	35.662183
1254.934238	171306.120215	35.667200
1256.216707	171619.854088	35.672218
1257.418052	171932.334561	35.677236
1258.850278	172241.454407	35.682253
1260.033773	172556.860653	35.687271
1261.433874	172869.479642	35.692288
1262.378466	173193.330210	35.697306
1263.485396	173514.465990	35.702324
1264.554374	173846.054050	35.707341
1265.752543	174190.592331	35.712359
1267.251315	174499.259334	35.717376
1268.329546	174839.342539	35.722394
1269.721707	175171.762193	35.727412
1271.336903	175487.459516	35.732429
1272.614445	175817.136080	35.737447
1274.518497	176154.566952	35.742464
1275.817109	176480.221680	35.747482
1277.185567	176799.509022	35.752500
1278.319175	177124.306959	35.757517
1279.323149	177452.554992	35.762535
1280.969618	177768.871201	35.767552
1281.906725	178106.855927	35.772570
1282.949897	178443.365980	35.777588
1284.480392	178781.270068	35.782605
1286.091211	179111.738777	35.787623
1287.228526	179446.272920	35.792640
1288.248402	179780.841366	35.797658
1289.895396	180110.231906	35.802676
1291.582577	180447.423320	35.807693
1292.242677	180786.639479	35.812711
1294.002772	181111.728042	35.817728
1295.276507	181449.311611	35.822746
1296.585927	181783.096603	35.827764
1297.741154	182121.503726	35.832781
1298.847957	182474.440860	35.837799
1300.470470	182815.428033	35.842816
1301.277179	183153.937454	35.847834
1302.759242	183490.560656	35.852852
1304.198314	183839.961727	35.857869
1304.876614	184192.638413	35.862887
1306.564138	184540.848061	35.867904
1307.789842	184892.855161	35.872922
1308.721467	185243.491506	35.877940
1310.152568	185606.918280	35.882957
1311.260855	185957.974342	35.887975
1312.722443	186317.707174	35.892992
1314.055886	186679.684816	35.898010
1315.547017	187031.611164	35.903028
1316.939449	187390.816608	35.908045
1318.349281	187757.053636	35.913063
1319.914697	188107.629032	35.918080
1321.249047	188453.103865	35.923098
1322.182735	188803.280109	35.928116
1323.627667	189162.577072	35.933133
1324.798317	189532.584344	35.938151
1326.485360	189893.115319	35.943168
1327.686601	190258.387404	35.948186
1328.816294	190603.617046	35.953204
1330.463104	190957.509623	35.958221
1331.758876	191313.950335	35.963239
1333.416194	191663.999108	35.968256
1334.730055	192028.057703	35.973274
1335.834707	192379.915651	35.978292
1337.295244	192715.633037	35.983309
1338.071414	193060.452985	35.988327
1339.593097	193398.944198	35.993344
1340.956572	193737.425328	35.998362
1341.971530	194080.421717	36.003380
1343.643794	194421.686608	36.008397
1344.765348	194781.388412	36.013415
1346.173386	195125.658715	36.018432
1347.182317	195481.549281	36.023450
1348.315447	195854.483615	36.028468
1349.552838	196203.294777	36.033485
1350.903205	196577.517832	36.038503
1351.881061	196937.801605	36.043520
1353.318499	197315.137668	36.048538
1354.257104	197697.039774	36.053556
1355.789829	198082.058058	36.058573
1356.889567	198460.903821	36.063591
1358.592534	198853.414370	36.068608
1359.739041	199241.829479	36.073626
1360.749886	199623.743576	36.078644
1362.017076	200024.229788	36.083661
1363.630063	200431.314025	36.088679
1364.760975	200828.628105	36.093696
1366.311879	201236.641532	36.098714
1367.176358	201649.849161	36.103732
1368.763804	202052.211563	36.108749
1370.043828	202486.063280	36.113767
1371.201582	202889.491735	36.118784
1372.635950	203315.806791	36.123802
1374.041925	203732.758986	36.128820
1375.542732	204145.736591	36.133837
1377.078977	204583.317032	36.138855
1378.449835	205000.053799	36.143872
1380.133270	205417.312713	36.148890
1381.099509	205848.163839	36.153908
1382.915795	206266.103939	36.158925
1384.097577	206696.860902	36.163943
1385.323708	207132.120504	36.168960
1387.078547	207558.216793	36.173978
1388.480508	207984.627627	36.178996
1390.197145	208418.467652	36.184013
1391.219097	208843.168269	36.189031
1392.511698	209270.581878	36.194048
1394.427790	209699.951908	36.199066
1395.703296	210132.337726	36.204084
1397.256613	210549.988717	36.209101
1398.477172	210987.733916	36.214119
1400.217257	211419.935621	36.219136
1402.107321	211842.807236	36.224154
1403.099269	212272.952789	36.229172
1404.634663	212693.715861	36.234189
1406.035247	213128.318836	36.239207
1407.333654	213546.966535	36.244224
1408.731829	213963.822037	36.249242
1409.850674	214404.725456	36.254260
1411.536544	214830.934360	36.259277
1412.765624	215265.677852	36.264295
1414.207792	215691.423134	36.269312
1416.329924	216109.515255	36.274330
1417.826861	216550.442999	36.279348
1419.565942	216957.275011	36.284365
1420.448960	217390.688843	36.289383
1421.957794	217800.991171	36.294400
1423.696268	218220.070374	36.299418
1425.053801	218642.871553	36.304436
1426.856506	219055.441941	36.309453
1428.033706	219463.240866	36.314471
1429.360768	219893.392495	36.319488
1430.562811	220333.395725	36.324506
1431.741366	220730.303741	36.329524
1433.192177	221139.715202	36.334541
1434.489914	221553.242715	36.339559
1436.091225	221941.246928	36.344576
1438.061471	222350.171046	36.349594
1439.437221	222759.804411	36.354612
1440.555923	223157.874441	36.359629
1442.092968	223554.454547	36.364647
1443.641990	223968.686493	36.369664
1445.137684	224369.264007	36.374682
1446.403655	224791.267069	36.379700
1447.846470	225193.786577	36.384717
1448.864110	225623.504306	36.389735
1450.009218	226046.801890	36.394752
1451.906893	226464.160282	36.399770
1452.763207	226906.456744	36.404788
1454.590348	227326.496749	36.409805
1455.750953	227759.475154	36.414823
1457.128677	228203.773054	36.419840
1458.503751	228618.024626	36.424858
1459.936439	229079.918812	36.429876
1461.421083	229514.246759	36.434893
1462.912709	229960.157565	36.439911
1464.410273	230414.400237	36.444928
1466.070424	230859.752820	36.449946
1467.463264	231306.954407	36.454964
1468.878916	231759.157608	36.459981
1470.445483	232206.917617	36.464999
1471.962149	232649.759491	36.470016
1473.765872	233108.761145	36.475034
1474.968064	233565.374183	36.480052
1476.512508	234007.402701	36.485069
1477.902118	234474.706810	36.490087
1479.185754	234942.614036	36.495104
1481.189947	235378.880703	36.500122
1482.849493	235850.487949	36.505140
1483.938961	236315.967261	36.510157
1485.245089	236761.954540	36.515175
1486.730951	237230.927174	36.520192
1488.531216	237690.526779	36.525210
1490.039045	238148.753332	36.530228
1491.674404	238607.620448	36.535245
1493.383170	239070.871110	36.540263
1494.741681	239529.405144	36.545280
1496.286916	239987.299808	36.550298
1497.640062	240474.007739	36.555316
1498.939597	240926.458261	36.560333
1500.675006	241395.044422	36.565351
1501.942281	241864.521737	36.570368
1503.943850	242314.852610	36.575386
1505.560765	242792.352134	36.580404
1507.339705	243246.227125	36.585421
1509.067166	243710.145444	36.590439
1510.438856	244168.890457	36.595456
1511.653728	244613.233573	36.600474
1513.252054	245077.963247	36.605492
1514.842128	245519.908980	36.610509
1517.093702	245979.883769	36.615527
1518.779398	246432.611321	36.620544
1520.415567	246874.500801	36.625562
1522.086847	247329.391358	36.630580
1523.417686	247766.455204	36.635597
1525.234331	248214.438915	36.640615
1526.257394	248654.145840	36.645632
1527.999872	249078.315072	36.650650
1529.500746	249520.992606	36.655668
1530.924520	249953.141173	36.660685
1532.002088	250383.162701	36.665703
1533.352503	250808.922775	36.670720
1534.860506	251235.825825	36.675738
1536.630624	251675.463784	36.680756
1537.588969	252100.883376	36.685773
1539.465192	252536.897407	36.690791
1540.835349	252986.179542	36.695808
1542.390720	253420.494447	36.700826
1543.189414	253875.714332	36.705844
1544.642108	254335.678657	36.710861
1546.163221	254790.373561	36.715879
1547.091594	255258.122207	36.720896
1548.997174	255714.888127	36.725914
1550.134369	256187.505694	36.730932
1551.667706	256674.919051	36.735949
1553.060998	257154.455332	36.740967
1554.438010	257636.102970	36.745984
1556.310782	258123.410125	36.751002
1558.063154	258617.316749	36.756020
1559.274692	259111.007896	36.761037
1561.164569	259605.755763	36.766055
1562.683401	260100.056853	36.771072
1564.448193	260592.208920	36.776090
1565.744868	261092.948340	36.781108
1567.694228	261591.827216	36.786125
1569.084656	262078.401449	36.791143
1571.243891	262564.899557	36.796160
1572.864864	263066.169471	36.801178
1574.763762	263564.167166	36.806196
1576.130785	264057.857679	36.811213
1578.101006	264551.397659	36.816231
1579.585175	265038.666794	36.821248
1581.220079	265518.696287	36.826266
1582.743029	266019.142767	36.831284
1584.035202	266522.091108	36.836301
1585.715223	267016.617448	36.841319
1587.190077	267529.111895	36.846336
1588.841828	268019.348968	36.851354
1590.413789	268530.784975	36.856372
1592.007394	269034.367354	36.861389
1593.985241	269534.659629	36.866407
1595.507364	270053.570772	36.871424
1597.318480	270545.252399	36.876442
1598.589719	271052.873977	36.881460
1599.712744	271567.632180	36.886477
1601.482714	272071.435896	36.891495
1603.204516	272599.074743	36.896512
1604.578583	273109.699453	36.901530
1606.299682	273625.397477	36.906548
1607.750992	274155.999778	36.911565
1609.527198	274659.849308	36.916583
1611.035253	275192.752048	36.921600
1612.635379	275703.589126	36.926618
1614.415926	276229.484598	36.931636
1616.034067	276749.004382	36.936653
1618.496393	277267.443933	36.941671
1619.197787	277791.888471	36.946688
1620.606136	278318.704647	36.951706
1622.219649	278844.672903	36.956724
1623.919065	279375.375974	36.961741
1625.299637	279899.805225	36.966759
1627.043103	280435.197821	36.971776
1628.597791	280964.930123	36.976794
1629.777578	281497.745722	36.981812
1631.397931	282048.319316	36.986829
1633.281637	282586.299378	36.991847
1634.239872	283135.073912	36.996864
1636.003469	283668.701533	37.001882
1637.874828	284191.768112	37.006900
1639.512926	284710.197724	37.011917
1641.584686	285221.492608	37.016935
1643.255890	285745.959111	37.021952
1644.685636	286282.783383	37.026970
1646.237249	286799.620409	37.031988
1647.779583	287324.382405	37.037005
1649.790589	287850.360734	37.042023
1650.980518	288386.404452	37.047040
1652.858362	288924.593402	37.052058
1654.073723	289455.777443	37.057076
1655.831225	289997.563724	37.062093
1657.361994	290552.923795	37.067111
1658.838201	291095.742799	37.072128
1660.647854	291640.054018	37.077146
1662.167485	292203.334009	37.082164
1664.186217	292757.537571	37.087181
1666.012072	293305.318943	37.092199
1667.780769	293858.542926	37.097216
1669.241546	294407.421066	37.102234
1671.767560	294956.527369	37.107252
1673.172356	295513.181990	37.112269
1675.457485	296074.286028	37.117287
1677.146835	296617.274335	37.122304
1679.016901	297153.601050	37.127322
1681.047993	297698.458113	37.132340
1682.874492	298228.818052	37.137357
1684.659704	298765.430325	37.142375
1686.085793	299318.963882	37.147392
1687.495657	299852.127590	37.152410
1689.477010	300402.922380	37.157428
1690.991615	300952.165734	37.162445
1692.943227	301492.724052	37.167463
1694.451887	302039.752824	37.172480
1696.509549	302579.601992	37.177498
1697.605107	303122.908600	37.182516
1699.675667	303689.239268	37.187533
1701.380335	304238.610656	37.192551
1702.524528	304793.709485	37.197568
1704.012290	305340.900600	37.202586
1706.001197	305917.720205	37.207604
1707.561821	306489.933773	37.212621
1709.636234	307041.640017	37.217639
1711.038388	307606.126551	37.222656
1712.510239	308173.188351	37.227674
1714.329342	308742.525570	37.232692
1715.919231	309320.988545	37.237709
1717.608164	309884.015953	37.242727
1719.429194	310473.683143	37.247744
1720.854009	311054.802411	37.252762
1722.444354	311645.362633	37.257780
1724.247332	312230.804415	37.262797
1725.560949	312816.779710	37.267815
1727.523103	313414.528340	37.272832
1728.979395	314001.156846	37.277850
1730.652886	314592.569942	37.282868
1732.436742	315209.785991	37.287885
1734.796905	315794.956394	37.292903
1736.483576	316391.431891	37.297920
1738.020226	316981.451952	37.302938
1739.750372	317581.389448	37.307956
1742.208143	318152.279217	37.312973
1744.442771	318721.728425	37.317991
1746.483792	319312.585560	37.323008
1748.126352	319888.318751	37.328026
1749.641721	320460.360857	37.333044
1750.998309	321049.919450	37.338061
1752.623522	321612.030869	37.343079
1754.398054	322169.618635	37.348096
1755.481997	322744.911846	37.353114
1757.253397	323307.187931	37.358132
1758.709728	323893.454761	37.363149
1760.604328	324471.874427	37.368167
1762.782936	325047.931484	37.373184
1764.251234	325631.489036	37.378202
1765.775752	326207.719586	37.383220
1767.481022	326811.335895	37.388237
1768.995647	327396.164150	37.393255
1770.528823	327983.522681	37.398272
1772.257867	328597.755536	37.403290
1773.971598	329200.585105	37.408308
1775.299896	329824.925407	37.413325
1777.071708	330436.161803	37.418343
1778.965323	331061.944388	37.423360
1780.470428	331699.488015	37.428378
1782.285480	332326.666173	37.433396
1784.212438	332958.388641	37.438413
1786.093570	333587.319055	37.443431
1788.079857	334225.465744	37.448448
1789.933323	334852.482458	37.453466
1792.150388	335495.323633	37.458484
1793.528958	336124.917330	37.463501
1795.337238	336774.461835	37.468519
1796.672798	337417.171730	37.473536
1798.260323	338081.790061	37.478554
1800.408556	338740.494498	37.483572
1801.715482	339403.568553	37.488589
1803.609144	340071.436399	37.493607
1805.461466	340737.652466	37.498624
1806.928426	341423.341432	37.503642
1808.770607	342091.851253	37.508660
1810.405636	342774.168956	37.513677
1812.526426	343462.793430	37.518695
1814.517383	344133.434099	37.523712
1816.349705	344830.285250	37.528730
1818.181572	345508.547609	37.533748
1820.093283	346187.980119	37.538765
1822.064890	346884.372440	37.543783
1823.954150	347575.565228	37.548800
1825.879026	348273.188349	37.553818
1827.875791	348948.506319	37.558836
1829.321593	349641.112076	37.563853
1831.178965	350344.323756	37.568871
1833.402286	351035.511193	37.573888
1834.957073	351729.386832	37.578906
1837.108710	352413.383067	37.583924
1839.000456	353113.348252	37.588941
1840.857889	353805.035300	37.593959
1843.212591	354482.926378	37.598976
1845.120167	355186.484576	37.603994
1846.686933	355861.032979	37.609012
1848.822555	356552.249634	37.614029
1850.675797	357242.080671	37.619047
1852.723035	357931.183341	37.624064
1854.194724	358618.771090	37.629082
1856.356679	359298.367969	37.634100
1858.362299	359990.310573	37.639117
1859.998445	360674.234088	37.644135
1862.477256	361351.156745	37.649152
1864.466728	362023.328235	37.654170
1866.586653	362702.875292	37.659188
1868.457679	363377.707556	37.664205
1870.180372	364042.886805	37.669223
1872.381762	364725.531680	37.674240
1873.750850	365389.300396	37.679258
1876.213586	366023.830119	37.684276
1877.920087	366676.663304	37.689293
1879.600950	367318.581411	37.694311
1881.502253	367954.135858	37.699328
1883.116198	368608.092850	37.704346
1885.189005	369239.893829	37.709364
1886.932197	369898.829676	37.714381
1889.223347	370553.427415	37.719399
1890.844874	371191.129271	37.724416
1892.769867	371854.895879	37.729434
1894.033898	372499.178144	37.734452
1895.871571	373154.311638	37.739469
1897.490735	373827.857867	37.744487
1899.398971	374487.952132	37.749504
1901.042451	375173.161463	37.754522
1902.491485	375856.208530	37.759540
1903.950548	376555.167815	37.764557
1905.799923	377250.599718	37.769575
1907.800255	377965.013285	37.774592
1909.754921	378670.847996	37.779610
1911.631901	379382.386971	37.784628
1913.083549	380108.258437	37.789645
1914.699849	380824.932902	37.794663
1916.633816	381554.066608	37.799680
1918.286950	382307.041371	37.804698
1920.283072	383032.912330	37.809716
1922.170126	383785.308019	37.814733
1923.788132	384547.467513	37.819751
1926.219544	385300.347364	37.824768
1927.732641	386057.088423	37.829786
1929.376895	386826.264293	37.834804
1932.108962	387591.566186	37.839821
1933.717712	388373.210047	37.844839
1935.890453	389135.524911	37.849856
1937.813943	389906.405951	37.854874
1940.365632	390669.305769	37.859892
1942.494664	391441.179946	37.864909
1944.661613	392209.758630	37.869927
1946.839775	392969.317514	37.874944
1948.914037	393733.183971	37.879962
1951.171815	394489.472830	37.884980
1953.309718	395252.226120	37.889997
1955.078288	396010.838928	37.895015
1957.136176	396767.103753	37.900032
1958.868754	397538.103223	37.905050
1960.528380	398292.088630	37.910068
1962.726988	399068.420459	37.915085
1964.334327	399836.947598	37.920103
1966.004751	400615.150257	37.925120
1968.083025	401398.637246	37.930138
1969.978554	402178.027879	37.935156
1972.116389	402959.562011	37.940173
1973.665861	403748.697672	37.945191
1976.044897	404518.771748	37.950208
1977.931513	405323.087325	37.955226
1980.230835	406095.665264	37.960244
1982.037777	406880.996790	37.965261
1983.602718	407680.660925	37.970279
1985.988679	408466.460094	37.975296
1987.865025	409270.992462	37.980314
1989.917886	410049.378150	37.985332
1991.941797	410848.823515	37.990349
1993.888071	411651.500600	37.995367
1995.886344	412439.250158	38.000384
1997.595439	413236.295327	38.005402
1999.605145	414032.101868	38.010420
2001.953342	414831.729387	38.015437
2003.507517	415619.939072	38.020455
2006.187413	416387.069243	38.025472
2007.819590	417162.758233	38.030490
2009.682154	417942.336944	38.035508
2011.742822	418710.513579	38.040525
2013.343054	419485.530228	38.045543
2015.561123	420264.448004	38.050560
2017.661831	421061.214175	38.055578
2019.387076	421835.252283	38.060596
2021.635767	422622.955268	38.065613
2022.833908	423422.277103	38.070631
2024.950332	424221.118030	38.075648
2026.554343	425026.322231	38.080666
2028.527048	425847.187406	38.085684
2031.018272	426662.825485	38.090701
2032.586558	427479.955649	38.095719
2034.536692	428298.008016	38.100736
2036.742691	429129.255576	38.105754
2038.408339	429963.246839	38.110772
2040.823766	430798.857339	38.115789
2042.462741	431644.590267	38.120807
2044.383383	432503.864115	38.125824
2046.515571	433354.871189	38.130842
2048.465246	434203.144077	38.135860
2050.799565	435055.777045	38.140877
2052.703575	435936.743691	38.145895
2055.055445	436790.221041	38.150912
2056.894271	437662.831902	38.155930
2059.201088	438530.473800	38.160948
2061.529214	439392.967756	38.165965
2063.519474	440254.877341	38.170983
2065.602579	441130.351110	38.176000
2067.724194	442012.666228	38.181018
2069.652091	442885.668070	38.186036
2071.944039	443764.090747	38.191053
2073.800039	444644.068302	38.196071
2076.300022	445528.407319	38.201088
2078.622935	446412.233906	38.206106
2080.540101	447291.184364	38.211124
2082.765035	448180.216562	38.216141
2085.015058	449072.597234	38.221159
2087.311311	449931.042300	38.226176
2089.249257	450817.685836	38.231194
2091.482561	451721.440668	38.236212
2094.097849	452581.395304	38.241229
2096.284894	453453.776370	38.246247
2099.990089	454292.239753	38.251264
2102.328680	455154.208054	38.256282
2104.183328	456004.235606	38.261300
2106.608432	456850.189974	38.266317
2108.070326	457712.196345	38.271335
2110.703394	458552.686520	38.276352
2112.692760	459394.259472	38.281370
2114.690889	460244.188861	38.286388
2116.766323	461084.716917	38.291405
2118.801485	461940.079512	38.296423
2120.539371	462782.867235	38.301440
2122.575680	463643.060483	38.306458
2124.827749	464502.271121	38.311476
2126.717224	465357.561756	38.316493
2128.550349	466224.955006	38.321511
2130.242311	467083.387484	38.326528
2132.256202	467954.363922	38.331546
2134.021245	468847.275304	38.336564
2136.297732	469721.161465	38.341581
2138.210297	470607.650536	38.346599
2140.155129	471499.146374	38.351616
2142.312953	472391.626653	38.356634
2144.209677	473272.841171	38.361652
2146.630918	474147.057230	38.366669
2148.735635	475015.879391	38.371687
2150.820721	475880.219117	38.376704
2153.249769	476746.684954	38.381722
2154.793393	477609.215525	38.386740
2157.536495	478474.690477	38.391757
2159.178019	479356.115758	38.396775
2161.605811	480228.783238	38.401792
2163.602741	481102.995403	38.406810
2165.858665	482002.424155	38.411828
2168.188764	482881.394804	38.416845
2170.175363	483769.569812	38.421863
2171.615606	484656.074462	38.426880
2174.099009	485565.841832	38.431898
2175.924116	486485.769270	38.436916
2178.144572	487397.001475	38.441933
2180.251701	488309.770618	38.446951
2182.662251	489239.858504	38.451968
2184.810623	490160.703038	38.456986
2187.012102	491086.790411	38.462004
2189.205464	492016.665973	38.467021
2191.209456	492952.478536	38.472039
2193.405584	493893.003278	38.477056
2196.146870	494824.807903	38.482074
2198.175976	495772.574893	38.487092
2200.273142	496718.461661	38.492109
2202.377958	497666.968856	38.497127
2204.810117	498611.585076	38.502144
2206.726279	499570.965135	38.507162
2208.993872	500520.294404	38.512180
2211.522476	501457.874140	38.517197
2213.761089	502435.802553	38.522215
2215.866845	503400.732573	38.527232
2218.124940	504356.956705	38.532250
2220.747734	505326.278715	38.537268
2223.037215	506287.832252	38.542285
2224.918616	507253.430725	38.547303
2227.127822	508224.615847	38.552320
2229.640428	509199.877762	38.557338
2231.531819	510177.855402	38.562356
2233.855405	511138.863779	38.567373
2235.811257	512134.810603	38.572391
2237.795651	513114.912682	38.577408
2240.271320	514111.860028	38.582426
2242.614918	515113.201796	38.587444
2244.776641	516098.432642	38.592461
2247.445994	517097.780066	38.597479
2249.549564	518091.966485	38.602496
2252.229093	519087.707753	38.607514
2254.230775	520076.845902	38.612532
2256.700005	521073.552287	38.617549
2258.372758	522078.940422	38.622567
2261.071440	523067.973016	38.627584
2263.643267	524077.917746	38.632602
2265.426644	525077.045543	38.637620
2267.918759	526070.349566	38.642637
2270.203168	527089.710615	38.647655
2272.502396	528079.892151	38.652672
2274.863576	529077.752912	38.657690
2277.217543	530091.308637	38.662708
2279.976430	531085.092107	38.667725
2282.013530	532079.582368	38.672743
2283.936961	533091.946375	38.677760
2286.831157	534086.512118	38.682778
2288.439918	535096.826351	38.687796
2290.916209	536110.148823	38.692813
2293.153861	537120.923487	38.697831
2295.148131	538118.029469	38.702848
2297.581152	539094.664046	38.707866
2299.290740	540087.302467	38.712884
2301.559784	541073.591033	38.717901
2303.790868	542062.584751	38.722919
2306.151169	543054.003696	38.727936
2308.317297	544040.857778	38.732954
2310.973317	545035.207766	38.737972
2313.069560	546019.620753	38.742989
2315.316289	547032.355732	38.748007
2317.559807	548026.712054	38.753024
2319.788152	549040.561196	38.758042
2322.078258	550054.476748	38.763060
2324.179565	551066.337720	38.768077
2326.661399	552094.752891	38.773095
2328.710088	553126.077970	38.778112
2331.380358	554152.145542	38.783130
2333.405532	555183.771032	38.788148
2335.646146	556224.027672	38.793165
2338.032726	557278.452796	38.798183
2340.300825	558330.151353	38.803200
2342.904388	559376.888155	38.808218
2344.825268	560433.754486	38.813236
2347.683789	561491.387002	38.818253
2349.964936	562559.228186	38.823271
2351.981185	563627.076840	38.828288
2354.492342	564680.944405	38.833306
2356.418643	565765.209135	38.838324
2359.146402	566852.164376	38.843341
2361.745723	567938.999665	38.848359
2364.390985	569017.852959	38.853376
2366.767893	570097.714619	38.858394
2369.169199	571198.014536	38.863412
2371.288242	572272.112955	38.868429
2373.684034	573365.851928	38.873447
2375.952182	574462.930759	38.878464
2378.652867	575553.369290	38.883482
2381.125903	576666.031616	38.888500
2383.307356	577766.902147	38.893517
2385.978481	578853.145516	38.898535
2388.234471	579953.309505	38.903552
2391.156108	581055.373286	38.908570
2393.039743	582157.811098	38.913588
2395.996600	583273.264512	38.918605
2398.402003	584359.219378	38.923623
2400.449895	585467.451781	38.928640
2403.099608	586566.158146	38.933658
2405.569311	587683.696440	38.938676
2407.681755	588792.818578	38.943693
2410.565274	589910.433910	38.948711
2412.476614	591035.724352	38.953728
2414.812497	592153.020831	38.958746
2417.449437	593271.416034	38.963764
2419.783104	594399.677646	38.968781
2421.975404	595526.251942	38.973799
2424.444282	596651.821597	38.978816
2427.078000	597768.139379	38.983834
2429.792758	598895.908258	38.988852
2431.991864	600030.615125	38.993869
2434.682740	601162.175742	38.998887
2437.023820	602301.946070	39.003904
2439.186023	603418.901935	39.008922
2441.369990	604557.874713	39.013940
2443.645786	605695.668192	39.018957
2446.414852	606836.370688	39.023975
2448.508458	607987.380745	39.028992
2451.198436	609138.226004	39.034010
2453.748934	610277.368115	39.039028
2455.903194	611404.102012	39.044045
2458.443076	612529.508808	39.049063
2460.668961	613649.951965	39.054080
2463.222736	614761.925437	39.059098
2465.212127	615870.379864	39.064116
2467.604115	616995.410470	39.069133
2470.144818	618130.503051	39.074151
2472.622195	619260.339234	39.079168
2474.992515	620380.028005	39.084186
2477.044304	621528.948389	39.089204
2479.395851	622688.244956	39.094221
2481.965897	623837.786046	39.099239
2484.178514	624994.610147	39.104256
2486.464178	626171.785037	39.109274
2488.597637	627342.361171	39.114292
2490.880398	628517.430907	39.119309
2493.721178	629701.770187	39.124327
2496.157126	630907.321291	39.129344
2498.624729	632105.189320	39.134362
2500.889675	633301.407121	39.139380
2503.310587	634519.931255	39.144397
2505.806693	635735.156490	39.149415
2507.750972	636969.250035	39.154432
2510.744523	638195.737607	39.159450
2513.130715	639446.284581	39.164468
2515.439502	640677.532124	39.169485
2518.332893	641929.142139	39.174503
2520.352874	643190.421767	39.179520
2523.733736	644435.110603	39.184538
2526.581795	645686.817648	39.189556
2528.697696	646950.858686	39.194573
2531.302672	648203.841407	39.199591
2533.756130	649464.371471	39.204608
2536.712725	650743.653418	39.209626
2538.950082	652018.055927	39.214644
2541.308138	653281.361755	39.219661
2544.060276	654542.548797	39.224679
2546.883670	655833.209159	39.229696
2549.115808	657120.709810	39.234714
2551.947177	658404.506487	39.239732
2554.302837	659683.382651	39.244749
2556.641163	660961.845514	39.249767
2559.172666	662272.821866	39.254784
2562.198499	663570.794944	39.259802
2564.872726	664860.637652	39.264820
2567.524500	666143.244044	39.269837
2570.239588	667438.508158	39.274855
2572.943826	668748.526286	39.279872
2575.520881	670035.649325	39.284890
2578.011892	671324.950369	39.289908
2580.344632	672640.711742	39.294925
2583.333503	673937.632182	39.299943
2585.813968	675247.236730	39.304960
2588.507510	676554.734091	39.309978
2591.043229	677865.951950	39.314996
2593.323084	679172.902091	39.320013
2595.909335	680481.854061	39.325031
2598.175875	681816.114142	39.330048
2600.480736	683131.643630	39.335066
2602.847737	684469.725369	39.340084
2605.564874	685799.209780	39.345101
2608.295759	687139.919938	39.350119
2610.804850	688472.723163	39.355136
2613.649970	689805.523174	39.360154
2616.506246	691138.074961	39.365172
2619.035110	692475.595297	39.370189
2621.927491	693797.125713	39.375207
2624.972216	695130.641045	39.380224
2627.531979	696444.838218	39.385242
2630.386752	697752.939271	39.390260
2632.674913	699030.737682	39.395277
2635.599637	700304.923711	39.400295
2638.266761	701600.088289	39.405312
2640.790514	702866.283627	39.410330
2643.558344	704153.617618	39.415348
2645.506155	705447.289277	39.420365
2648.462874	706746.349582	39.425383
2650.687817	708041.817805	39.430400
2652.784215	709349.743987	39.435418
2655.529618	710661.128200	39.440436
2658.171242	711984.461056	39.445453
2660.456004	713322.996309	39.450471
2662.914844	714664.955587	39.455488
2665.426815	716002.931989	39.460506
2667.850733	717349.619007	39.465524
2670.347577	718730.814009	39.470541
2673.114818	720086.209465	39.475559
2675.355791	721463.186895	39.480576
2677.893150	722852.400473	39.485594
2680.702468	724246.578442	39.490612
2683.133135	725640.534662	39.495629
2685.817345	727049.191254	39.500647
2688.127290	728477.733762	39.505664
2690.937751	729899.471641	39.510682
2693.823634	731312.056712	39.515700
2696.373618	732756.658528	39.520717
2698.941986	734192.653585	39.525735
2701.809959	735642.269035	39.530752
2704.217367	737102.560923	39.535770
2707.255280	738553.647725	39.540788
2709.917187	740020.868763	39.545805
2713.052157	741462.626368	39.550823
2716.328270	742936.758045	39.555840
2718.929366	744391.095331	39.560858
2721.662734	745849.827754	39.565876
2723.972036	747323.249967	39.570893
2727.231311	748781.005847	39.575911
2730.051537	750254.728341	39.580928
2732.579330	751730.536057	39.585946
2735.497704	753203.830769	39.590964
2738.185788	754691.709723	39.595981
2740.659416	756152.790854	39.600999
2743.679632	757648.760125	39.606016
2746.501047	759143.091146	39.611034
2749.311032	760615.719884	39.616052
2751.911617	762100.794334	39.621069
2754.750510	763589.917236	39.626087
2757.556059	765086.966879	39.631104
2760.152295	766574.555873	39.636122
2763.297203	768076.461820	39.641140
2766.014154	769573.465798	39.646157
2768.710285	771059.899186	39.651175
2771.653619	772548.156294	39.656192
2774.683067	774047.989832	39.661210
2777.993185	775541.036681	39.666228
2780.653891	777028.975645	39.671245
2783.698237	778503.683857	39.676263
2786.405410	780001.174194	39.681280
2789.229769	781481.844863	39.686298
2792.164850	782961.016961	39.691316
2795.016588	784453.539332	39.696333
2798.281436	785927.877973	39.701351
2800.955558	787410.053960	39.706368
2803.503478	788886.844144	39.711386
2806.594495	790354.806992	39.716404
2809.118254	791846.968054	39.721421
2811.814779	793303.896842	39.726439
2814.768729	794750.194155	39.731456
2817.093410	796183.170670	39.736474
2819.816028	797624.260989	39.741492
2822.174694	799065.701771	39.746509
2825.030414	800513.909468	39.751527
2827.993881	801975.403197	39.756544
2830.300400	803426.763730	39.761562
2833.162257	804889.713198	39.766580
2835.256753	806367.297868	39.771597
2838.039722	807840.147663	39.776615
2840.841378	809327.197136	39.781632
2843.001075	810831.672965	39.786650
2845.908531	812326.945165	39.791668
2848.726371	813853.805197	39.796685
2851.572175	815361.802808	39.801703
2854.716962	816899.495062	39.806720
2857.163514	818450.278383	39.811738
2860.050166	819982.032108	39.816756
2862.528013	821536.778741	39.821773
2865.447827	823099.431364	39.826791
2868.332972	824666.793492	39.831808
2871.093237	826251.066701	39.836826
2874.191344	827840.509060	39.841844
2877.126612	829421.014008	39.846861
2880.055206	830996.313160	39.851879
2883.238234	832597.886600	39.856896
2885.616246	834196.664435	39.861914
2888.962905	835797.273234	39.866932
2891.832602	837399.072021	39.871949
2895.080179	838990.966970	39.876967
2897.979474	840596.439324	39.881984
2900.998432	842204.065990	39.887002
2904.283724	843799.035261	39.892020
2906.857051	845402.034394	39.897037
2910.097809	847018.904657	39.902055
2913.268842	848632.649575	39.907072
2915.849503	850239.177702	39.912090
2919.038525	851851.604063	39.917108
2921.759038	853476.315395	39.922125
2924.625330	855095.820160	39.927143
2927.587652	856720.806278	39.932160
2930.206045	858356.871619	39.937178
2933.201730	859991.372245	39.942196
2936.364904	861628.124871	39.947213
2939.035250	863272.955618	39.952231
2942.113628	864899.923171	39.957248
2944.576220	866556.694559	39.962266
2947.616364	868206.716294	39.967284
2950.486189	869875.588513	39.972301
2953.373406	871540.992360	39.977319
2956.359037	873192.364276	39.982336
2959.123164	874860.444652	39.987354
2962.040943	876546.897414	39.992372
2964.698852	878217.437738	39.997389
2967.744078	879888.601936	40.002407
2971.040936	881572.493180	40.007424
2973.966274	883266.205656	40.012442
2977.059330	884950.511679	40.017460
2979.844512	886636.313039	40.022477
2982.552801	888342.782640	40.027495
2985.769753	890024.823655	40.032512
2988.693839	891723.984571	40.037530
2991.808510	893414.894323	40.042548
2994.507810	895113.667082	40.047565
2997.206490	896817.719055	40.052583
3000.666146	898524.026718	40.057600
3002.979184	900245.618803	40.062618
3006.108260	901937.462555	40.067636
3008.633311	903619.749657	40.072653
3011.665363	905305.299713	40.077671
3014.603809	906982.177304	40.082688
3017.093022	908664.108479	40.087706
3020.137220	910342.361593	40.092724
3023.061776	912053.008840	40.097741
3025.734144	913763.263766	40.102759
3028.830480	915465.710694	40.107776
3031.677917	917184.576522	40.112794
3034.176717	918910.545560	40.117812
3037.440905	920646.689492	40.122829
3040.304077	922383.399979	40.127847
3043.177041	924123.293008	40.132864
3046.461747	925885.382246	40.137882
3049.351128	927637.755098	40.142900
3052.106817	929407.978329	40.147917
3054.979537	931189.092461	40.152935
3058.103441	932961.715198	40.157952
3060.836130	934769.426927	40.162970
3063.964301	936574.253695	40.167988
3066.800402	938387.599456	40.173005
3069.646053	940213.611771	40.178023
3073.036982	942047.406087	40.183040
3075.694675	943885.072397	40.188058
3078.859982	945725.444341	40.193076
3081.947241	947568.994952	40.198093
3084.812113	949431.304636	40.203111
3088.136111	951294.008964	40.208128
3090.963018	953163.654531	40.213146
3094.001410	955041.107979	40.218164
3096.815900	956985.160523	40.223181
3099.508146	958932.588274	40.228199
3103.006340	960879.421485	40.233216
3105.804828	962835.094174	40.238234
3108.769894	964814.889430	40.243252
3111.896623	966785.578177	40.248269
3114.632621	968764.051581	40.253287
3118.325020	970750.469252	40.258304
3121.186611	972749.896702	40.263322
3124.507131	974733.922659	40.268340
3127.937220	976720.752982	40.273357
3131.319101	978729.024024	40.278375
3134.547282	980709.531571	40.283392
3138.202031	982713.337113	40.288410
3141.631464	984703.138623	40.293428
3145.312976	986687.922066	40.298445
3148.325675	988665.703169	40.303463
3151.817674	990650.109227	40.308480
3154.531870	992638.228448	40.313498
3157.694667	994626.744246	40.318516
3161.048510	996605.691158	40.323533
3163.752017	998594.446015	40.328551
3167.148351	1000596.271415	40.333568
3170.342074	1002598.780818	40.338586
3172.948375	1004596.797282	40.343604
3176.001677	1006611.392801	40.348621
3178.711124	1008618.830615	40.353639
3181.888197	1010629.547010	40.358656
3184.524545	1012673.734831	40.363674
3187.456851	1014706.091788	40.368692
3190.589300	1016737.294002	40.373709
3193.340266	1018799.081159	40.378727
3196.675484	1020841.925449	40.383744
3199.556533	1022908.855042	40.388762
3202.771722	1024971.970389	40.393780
3205.974830	1027057.131033	40.398797
3208.959511	1029126.771560	40.403815
3212.421094	1031175.386578	40.408832
3215.515440	1033216.650019	40.413850
3218.664287	1035244.228037	40.418868
3222.013316	1037273.928371	40.423885
3224.836061	1039311.748639	40.428903
3228.151536	1041353.174110	40.433920
3231.373451	1043379.798322	40.438938
3234.240644	1045424.328148	40.443956
3237.378507	1047481.826206	40.448973
3240.188436	1049544.965366	40.453991
3243.308332	1051606.514416	40.459008
3246.465854	1053685.174857	40.464026
3249.632017	1055782.180747	40.469044
3253.129480	1057864.881944	40.474061
3256.146139	1059977.228474	40.479079
3259.190507	1062077.717766	40.484096
3262.246002	1064195.063466	40.489114
3264.968964	1066326.231364	40.494132
3268.548374	1068463.527722	40.499149
3271.864034	1070616.044376	40.504167
3274.902520	1072761.723303	40.509184
3278.187321	1074928.073725	40.514202
3281.168507	1077094.381523	40.519220
3284.468553	1079274.134887	40.524237
3287.993088	1081466.279475	40.529255
3290.898117	1083655.539999	40.534272
3294.187974	1085855.137574	40.539290
3297.566855	1088062.144575	40.544308
3301.345790	1090260.069319	40.549325
3304.681667	1092480.761389	40.554343
3308.617822	1094689.277517	40.559360
3311.657301	1096893.224063	40.564378
3315.203634	1099108.872966	40.569396
3318.729099	1101328.287714	40.574413
3321.725638	1103552.784763	40.579431
3325.079716	1105771.066299	40.584448
3328.586156	1108002.881014	40.589466
3331.578869	1110228.429616	40.594484
3335.343059	1112458.732488	40.599501
3338.695933	1114691.599680	40.604519
3342.153584	1116925.991153	40.609536
3345.494555	1119158.329569	40.614554
3348.667123	1121400.116391	40.619572
3352.386253	1123654.638189	40.624589
3355.698643	1125891.668569	40.629607
3358.909785	1128128.346361	40.634624
3362.110625	1130373.947348	40.639642
3365.531546	1132630.979739	40.644660
3368.871320	1134889.814354	40.649677
3372.329749	1137145.490525	40.654695
3375.847976	1139406.633835	40.659712
3379.163503	1141667.507719	40.664730
3382.031162	1143927.394894	40.669748
3385.518441	1146190.940489	40.674765
3388.670724	1148470.673609	40.679783
3392.200510	1150740.953236	40.684800
3395.232957	1153023.175992	40.689818
3398.456214	1155317.211584	40.694836
3401.697957	1157606.564302	40.699853
3404.629874	1159922.501011	40.704871
3408.130787	1162214.891586	40.709888
3411.467640	1164530.610100	40.714906
3414.540863	1166850.526034	40.719924
3417.724746	1169167.041147	40.724941
3420.838858	1171504.930014	40.729959
3423.937289	1173844.876497	40.734976
3427.299696	1176189.931790	40.739994
3430.233114	1178542.362175	40.745012
3433.469642	1180878.699151	40.750016
3436.835631	1183175.377946	40.755021
3440.446752	1185420.768979	40.760026
3443.858331	1187595.077387	40.765031
3446.561572	1189701.012806	40.770036
3449.751667	1191721.455953	40.775040
3453.018706	1193681.085003	40.780045
3456.142322	1195541.138320	40.785050
3458.996958	1197323.985395	40.790055
3461.708503	1199034.844825	40.795060
3464.124944	1200659.932372	40.800064
3466.598109	1202227.304588	40.805069
3468.914348	1203706.961381	40.810074
3471.660657	1205112.281370	40.815079
3473.827944	1206447.051266	40.820084
3475.378519	1207721.540815	40.825088
3477.227491	1208936.299530	40.830093
3479.430033	1210071.233458	40.835098
3481.733256	1211159.382556	40.840103
3483.218739	1212183.522662	40.845108
3485.243309	1213140.942656	40.850112
3486.919258	1214044.454239	40.855117
3488.490738	1214883.757849	40.860122
3490.390858	1215667.603905	40.865127
3491.781106	1216419.624090	40.870132
3493.185321	1217091.601164	40.875136
3494.288042	1217726.897466	40.880141
3495.814336	1218319.332174	40.885146
3496.995783	1218868.112203	40.890151
3497.926373	1219386.598667	40.895156
3499.205396	1219855.641375	40.900160
3500.167412	1220299.374364	40.905165
3501.328604	1220688.105225	40.910170
3502.512491	1221050.646977	40.915175
3503.269562	1221372.601127	40.920180
3504.742682	1221669.385317	40.925184
3505.016261	1221928.617409	40.930189
3505.793394	1222155.065922	40.935194
3506.508771	1222366.759058	40.940199
3507.402539	1222542.834114	40.945204
3508.272628	1222700.137025	40.950208
3508.476265	1222838.215106	40.955213
3509.046726	1222934.675705	40.960218
3509.774078	1223012.713360	40.965223
3510.628377	1223095.771194	40.970228
3510.892018	1223136.066031	40.975232
3511.609177	1223164.427325	40.980237
3512.129280	1223162.754436	40.985242
3513.132580	1223166.044189	40.990247
3513.032742	1223133.566376	40.995252
3513.483537	1223076.533221	41.000256
3514.026520	1223017.616703	41.005261
3514.252835	1222944.278018	41.010266
3514.691045	1222857.550054	41.015271
3514.911403	1222749.378671	41.020276
3515.259130	1222635.767737	41.025280
3515.926903	1222511.829069	41.030285
3516.223284	1222368.990616	41.035290
3516.553216	1222226.702976	41.040295
3516.420759	1222053.480527	41.045300
3516.865479	1221875.393825	41.050304
3517.059199	1221706.775752	41.055309
3517.624370	1221506.239967	41.060314
3517.538206	1221308.699210	41.065319
3517.424830	1221117.040219	41.070324
3517.926637	1220892.390330	41.075328
3517.943410	1220682.570780	41.080333
3518.087896	1220462.538339	41.085338
3518.432993	1220231.158542	41.090343
3518.536062	1219993.361242	41.095348
3518.557901	1219747.717497	41.100352
3518.665896	1219517.185232	41.105357
3518.730896	1219267.680121	41.110362
3519.327553	1219007.982562	41.115367
3519.261799	1218753.333994	41.120372
3519.562946	1218467.770360	41.125376
3519.504611	1218197.297903	41.130381
3519.590199	1217919.870557	41.135386
3519.878014	1217638.468819	41.140391
3519.596747	1217352.284251	41.145396
3519.951648	1217067.755081	41.150400
3519.819658	1216775.343432	41.155405
3519.880420	1216482.509276	41.160410
3520.037239	1216183.564824	41.165415
3520.132622	1215881.807727	41.170420
3519.944783	1215573.533465	41.175424
3519.898033	1215277.000757	41.180429
3520.048449	1214984.813995	41.185434
3520.798212	1214663.330408	41.190439
3520.476199	1214350.514881	41.195444
3520.869550	1214019.508759	41.200448
3520.326891	1213711.741690	41.205453
3520.482656	1213373.810293	41.210458
3520.522234	1213042.050639	41.215463
3520.314209	1212719.853950	41.220468
3520.585994	1212398.587209	41.225472
3520.348587	1212069.523590	41.230477
3520.404084	1211741.139209	41.235482
3520.747882	1211420.079850	41.240487
3520.616534	1211085.787979	41.245492
3520.798993	1210737.850256	41.250496
3520.882700	1210400.763715	41.255501
3520.254158	1210079.125026	41.260506
3520.534859	1209742.711587	41.265511
3520.674561	1209408.171784	41.270516
3520.621112	1209069.428446	41.275520
3520.984726	1208729.470333	41.280525
3520.496577	1208388.225240	41.285530
3520.439167	1208043.702303	41.290535
3520.446874	1207716.378477	41.295540
3520.228981	1207369.869821	41.300544
3520.474020	1207041.339803	41.305549
3520.525547	1206702.609905	41.310554
3520.720642	1206353.528911	41.315559
3520.460674	1206014.804846	41.320564
3520.666566	1205669.329332	41.325568
3520.506786	1205323.797059	41.330573
3520.521618	1204971.934327	41.335578
3520.882759	1204629.830397	41.340583
3520.319866	1204288.605592	41.345588
3520.402194	1203948.376537	41.350592
3520.632402	1203604.351263	41.355597
3520.515916	1203243.955676	41.360602
3520.832944	1202897.993977	41.365607
3520.467672	1202561.402765	41.370612
3520.637663	1202202.574419	41.375616
3520.558240	1201863.265129	41.380621
3520.603638	1201507.315428	41.385626
3520.626901	1201146.937164	41.390631
3520.539362	1200799.962987	41.395636
3520.555921	1200444.507110	41.400640
3520.319096	1200101.168160	41.405645
3520.518128	1199737.942043	41.410650
3520.790330	1199398.693499	41.415655
3520.512154	1199047.317170	41.420660
3520.807356	1198689.911597	41.425664
3520.506808	1198324.322359	41.430669
3520.246205	1197975.778634	41.435674
3520.330335	1197617.113444	41.440679
3520.397420	1197269.218637	41.445684
3520.151332	1196911.121729	41.450688
3520.177841	1196561.214811	41.455693
3520.052160	1196210.182771	41.460698
3520.418114	1195859.796832	41.465703
3519.877458	1195502.589222	41.470708
3520.475923	1195151.741327	41.475712
3520.119553	1194802.341311	41.480717
3519.974329	1194449.502443	41.485722
3520.217184	1194091.880204	41.490727
3520.073150	1193755.896758	41.495732
3520.570243	1193396.963607	41.500736
3520.015752	1193041.090356	41.505741
3520.047623	1192690.262225	41.510746
3519.950894	1192335.298142	41.515751
3519.860030	1191985.193794	41.520756
3519.886261	1191627.530334	41.525760
3519.897675	1191286.099169	41.530765
3519.947539	1190930.920409	41.535770
3520.058527	1190574.767454	41.540775
3519.852872	1190227.099985	41.545780
3519.723132	1189875.355349	41.550784
3519.564421	1189526.599193	41.555789
3519.603127	1189173.275196	41.560794
3519.860078	1188806.730791	41.565799
3519.614700	1188457.070719	41.570804
3519.833445	1188117.652210	41.575808
3519.603221	1187767.943042	41.580813
3519.492418	1187408.129594	41.585818
3519.564161	1187059.733231	41.590823
3519.349664	1186717.943379	41.595828
3519.497624	1186363.374959	41.600832
3519.443540	1186029.225035	41.605837
3519.447773	1185693.444936	41.610842
3519.641672	1185330.144763	41.615847
3519.314638	1184989.670305	41.620852
3519.491562	1184642.599086	41.625856
3519.392510	1184282.660499	41.630861
3518.969984	1183941.568363	41.635866
3519.523580	1183599.446143	41.640871
3519.013957	1183253.524115	41.645876
3518.986846	1182907.311311	41.650880
3519.062587	1182558.423209	41.655885
3519.015796	1182224.685466	41.660890
3518.984160	1181879.440128	41.665895
3519.192678	1181550.605764	41.670900
3519.220861	1181188.360417	41.675904
3518.938714	1180844.687873	41.680909
3519.080971	1180506.289403	41.685914
3519.299877	1180159.099439	41.690919
3519.028770	1179813.756110	41.695924
3519.133304	1179474.260774	41.700928
3518.745204	1179130.115479	41.705933
3518.349503	1178784.724233	41.710938
3518.547626	1178436.951649	41.715943
3518.566003	1178109.531890	41.720948
3518.682980	1177771.147769	41.725952
3518.880206	1177426.699041	41.730957
3518.627179	1177088.331414	41.735962
3518.757074	1176736.593500	41.740967
3518.500091	1176405.531359	41.745972
3518.712215	1176067.963012	41.750976
3518.671192	1175722.875280	41.755981
3518.484809	1175389.569341	41.760986
3518.680163	1175050.901080	41.765991
3518.403562	1174714.550706	41.770996
3518.359259	1174376.726379	41.776000
3518.442304	1174031.506075	41.781005
3518.273843	1173701.482827	41.786010
3518.160285	1173356.344427	41.791015
3517.930628	1173037.885960	41.796020
3518.015706	1172692.859471	41.801024
3518.086749	1172371.387615	41.806029
3518.093085	1172029.819320	41.811034
3518.179003	1171702.173815	41.816039
3517.935301	1171364.092645	41.821044
3518.068260	1171039.132974	41.826048
3517.781324	1170711.580958	41.831053
3517.592502	1170378.709371	41.836058
3517.824652	1170069.049760	41.841063
3517.665266	1169730.848835	41.846068
3517.699162	1169397.594935	41.851072
3517.800472	1169079.028836	41.856077
3517.626169	1168750.014083	41.861082
3517.805481	1168416.673625	41.866087
3517.831119	1168095.606323	41.871092
3517.636412	1167764.456526	41.876096
3517.624260	1167445.998265	41.881101
3517.739805	1167118.626405	41.886106
3517.650510	1166779.278795	41.891111
3517.280007	1166452.039627	41.896116
3517.733884	1166130.403414	41.901120
3517.636562	1165812.709378	41.906125
3517.246166	1165485.507400	41.911130
3517.348222	1165156.976244	41.916135
3516.807975	1164849.022969	41.921140
3516.748333	1164534.455909	41.926144
3517.350194	1164216.360878	41.931149
3517.310304	1163891.173739	41.936154
3517.321778	1163565.391181	41.941159
3517.066791	1163251.629326	41.946164
3517.062761	1162918.251831	41.951168
3517.124265	1162615.169420	41.956173
3516.646460	1162301.954209	41.961178
3516.940206	1161960.813657	41.966183
3516.809775	1161663.188104	41.971188
3516.811720	1161358.719897	41.976192
3517.153427	1161044.066020	41.981197
3516.646781	1160729.721996	41.986202
3516.507894	1160408.587884	41.991207
3516.476202	1160111.236001	41.996212
3516.445600	1159784.090930	42.001216
3516.625569	1159475.608397	42.006221
3516.265669	1159171.923577	42.011226
3516.482652	1158856.119036	42.016231
3516.504464	1158546.095189	42.021236
3516.296587	1158252.921728	42.026240
3516.549916	1157942.256756	42.031245
3516.379524	1157636.466075	42.036250
3516.528052	1157338.643666	42.041255
3516.281030	1157029.520243	42.046260
3516.435382	1156723.528338	42.051264
3516.273231	1156407.544359	42.056269
3516.164171	1156103.073111	42.061274
3516.040142	1155788.559128	42.066279
3515.565823	1155492.342808	42.071284
3515.861961	1155197.969717	42.076288
3516.157750	1154902.160970	42.081293
3515.969252	1154598.940280	42.086298
3516.001275	1154294.719520	42.091303
3515.942057	1153999.486224	42.096308
3516.188180	1153688.286999	42.101312
3516.071093	1153393.691697	42.106317
3515.615219	1153102.259079	42.111322
3515.848945	1152779.082458	42.116327
3515.720550	1152490.496291	42.121332
3515.776524	1152191.545528	42.126336
3516.014295	1151898.890720	42.131341
3515.537515	1151590.053218	42.136346
3515.642547	1151284.510284	42.141351
3515.296135	1150997.393064	42.146356
3515.254553	1150715.039227	42.151360
3515.763221	1150419.985052	42.156365
3515.333989	1150125.826438	42.161370
3515.247271	1149828.090836	42.166375
3515.339396	1149535.233994	42.171380
3515.460070	1149239.041071	42.176384
3515.326357	1148959.828757	42.181389
3515.094855	1148671.713368	42.186394
3515.652729	1148371.800083	42.191399
3515.074395	1148083.993903	42.196404
3515.297110	1147797.461238	42.201408
3515.313859	1147508.862468	42.206413
3515.217592	1147227.562558	42.211418
3515.305342	1146923.664744	42.216423
3514.921069	1146637.642867	42.221428
3514.654095	1146354.524015	42.226432
3515.138505	1146077.237013	42.231437
3514.916925	1145795.691881	42.236442
3515.117473	1145498.896700	42.241447
3515.039261	1145221.657446	42.246452
3514.817880	1144935.232139	42.251456
3515.022804	1144645.877095	42.256461
3514.635010	1144376.323250	42.261466
3514.799807	1144090.831420	42.266471
3514.878351	1143811.027273	42.271476
3514.693403	1143527.648554	42.276480
3514.412264	1143247.020412	42.281485
3514.266250	1142976.312262	42.286490
3514.496563	1142685.138773	42.291495
3514.581336	1142417.493570	42.296500
3514.502239	1142147.490697	42.301504
3514.490491	1141866.080993	42.306509
3514.326336	1141590.467562	42.311514
3514.226092	1141318.149336	42.316519
3514.328096	1141053.847263	42.321524
3514.195927	1140759.876462	42.326528
3514.393778	1140496.289727	42.331533
3514.022100	1140240.943259	42.336538
3514.517671	1139950.334649	42.341543
3514.138170	1139682.627599	42.346548
3514.314400	1139415.479747	42.351552
3514.434314	1139146.619528	42.356557
3514.003056	1138870.623785	42.361562
3514.420451	1138596.372063	42.366567
3514.451028	1138322.169861	42.371572
3513.838929	1138052.520469	42.376576
3513.811139	1137776.116513	42.381581
3513.809371	1137505.769249	42.386586
3514.099997	1137237.733365	42.391591
3514.017281	1136983.036653	42.396596
3513.992480	1136698.506368	42.401600
3513.971201	1136435.798100	42.406605
3513.736181	1136181.182915	42.411610
3513.730593	1135906.481941	42.416615
3513.983092	1135639.606035	42.421620
3513.782262	1135369.182662	42.426624
3513.544803	1135106.159269	42.431629
3513.533340	1134851.158536	42.436634
3513.632054	1134585.299687	42.441639
3513.421718	1134333.536170	42.446644
3513.587041	1134066.880524	42.451648
3513.809092	1133802.292022	42.456653
3513.251083	1133547.888683	42.461658
3513.375180	1133287.090600	42.466663
3513.566811	1133018.857969	42.471668
3513.292234	1132760.379891	42.476672
3513.633679	1132506.633671	42.481677
3513.136447	1132245.221670	42.486682
3513.332612	1131980.261651	42.491687
3513.093698	1131734.176276	42.496692
3513.007804	1131478.740821	42.501696
3513.229826	1131218.775494	42.506701
3512.764097	1130975.733660	42.511706
3513.054312	1130722.385967	42.516711
3512.794882	1130482.519291	42.521716
3512.903039	1130226.896708	42.526720
3512.960672	1129970.604731	42.531725
3512.670869	1129745.349444	42.536730
3512.724000	1129495.880142	42.541735
3512.622662	1129242.906793	42.546740
3512.612873	1128998.463550	42.551744
3512.439495	1128752.229425	42.556749
3512.465315	1128497.678377	42.561754
3512.453027	1128263.566493	42.566759
3512.541675	1128039.793288	42.571764
3512.530154	1127785.214344	42.576768
3512.643400	1127545.439230	42.581773
3512.835110	1127311.442124	42.586778
3512.791156	1127053.980285	42.591783
3512.788775	1126812.384056	42.596788
3512.769065	1126573.157813	42.601792
3512.620820	1126315.677488	42.606797
3512.490412	1126072.071107	42.611802
3512.724611	1125833.245510	42.616807
3512.227407	1125589.487216	42.621812
3512.265315	1125344.107323	42.626816
3512.685263	1125100.651366	42.631821
3512.170747	1124864.474738	42.636826
3512.380130	1124632.165060	42.641831
3512.220038	1124390.675398	42.646836
3512.376453	1124145.696685	42.651840
3512.387042	1123921.097284	42.656845
3512.143953	1123681.682961	42.661850
3511.996205	1123442.432553	42.666855
3512.078375	1123198.374387	42.671860
3512.186284	1122962.106222	42.676864
3512.215578	1122742.213528	42.681869
3512.125346	1122499.579696	42.686874
3512.238376	1122262.422977	42.691879
3512.246655	1122034.126979	42.696884
3511.756656	1121801.714124	42.701888
3512.275514	1121564.459590	42.706893
3512.155279	1121320.825039	42.711898
3512.133838	1121087.827878	42.716903
3511.988640	1120858.459499	42.721908
3511.820879	1120615.181508	42.726912
3512.061673	1120377.158251	42.731917
3511.881065	1120158.908020	42.736922
3512.053299	1119924.971145	42.741927
3511.847317	1119691.181575	42.746932
3511.722089	1119459.368736	42.751936
3511.787095	1119238.373485	42.756941
3511.567955	1119007.509070	42.761946
3511.469858	1118773.852152	42.766951
3511.888610	1118552.484530	42.771956
3511.576145	1118320.367376	42.776960
3511.738279	1118091.591869	42.781965
3511.418482	1117864.696248	42.786970
3511.614322	1117630.655177	42.791975
3511.721507	1117415.771086	42.796980
3511.136395	1117184.507150	42.801985
3511.170054	1116968.473731	42.806989
3511.455988	1116755.630190	42.811994
3511.700495	1116518.197058	42.816999
3511.257507	1116309.458538	42.822004
3510.997847	1116093.533447	42.827009
3511.364517	1115865.677578	42.832013
3511.210934	1115659.820813	42.837018
3511.279704	1115446.865738	42.842023
3511.208797	1115223.058119	42.847028
3511.193546	1115002.282529	42.852033
3511.359899	1114781.181939	42.857037
3511.292403	1114571.837211	42.862042
3511.507263	1114339.079280	42.867047
3511.376830	1114121.051269	42.872052
3511.283680	1113897.573363	42.877057
3511.256849	1113677.984694	42.882061
3511.262255	1113456.665304	42.887066
3511.226477	1113223.804904	42.892071
3510.990511	1113019.099998	42.897076
3511.313497	1112813.913753	42.902081
3511.004646	1112587.460379	42.907085
3510.876408	1112382.141197	42.912090
3510.191827	1112160.595855	42.917095
3510.387437	1111963.219215	42.922100
3510.543169	1111758.210933	42.927105
3511.038907	1111540.261077	42.932109
3510.758409	1111342.176899	42.937114
3510.806588	1111124.760867	42.942119
3510.578722	1110918.257329	42.947124
3510.462451	1110709.533141	42.952129
3510.400095	1110511.382390	42.957133
3510.420258	1110305.005244	42.962138
3510.376980	1110099.871035	42.967143
3510.434893	1109902.059672	42.972148
3510.454109	1109689.265895	42.977153
3510.621758	1109480.924340	42.982157
3510.156534	1109290.524535	42.987162
3510.411332	1109081.007960	42.992167
3510.413463	1108885.267928	42.997172
3510.318940	1108680.565180	43.002177
3510.450928	1108469.327053	43.007181
3510.625245	1108278.690634	43.012186
3510.620865	1108068.604615	43.017191
3510.374247	1107865.327674	43.022196
3510.123073	1107659.466387	43.027201
3510.457338	1107460.087775	43.032205
3510.144664	1107251.548033	43.037210
3510.089454	1107037.993325	43.042215
3510.058915	1106850.204154	43.047220
3510.183806	1106662.478311	43.052225
3509.867920	1106462.405999	43.057229
3509.973169	1106272.378243	43.062234
3510.154566	1106057.599858	43.067239
3509.831619	1105867.246372	43.072244
3509.651828	1105678.867971	43.077249
3509.917739	1105473.124365	43.082253
3509.459046	1105292.800262	43.087258
3509.754444	1105103.559462	43.092263
3509.753473	1104915.793454	43.097268
3509.709656	1104730.129217	43.102273
3509.537796	1104536.933978	43.107277
3509.500992	1104359.947700	43.112282
3509.551054	1104164.219072	43.117287
3509.501743	1103973.467012	43.122292
3509.385914	1103794.182564	43.127297
3509.602657	1103604.042312	43.132301
3509.075675	1103417.266032	43.137306
3509.372890	1103235.411064	43.142311
3509.431989	1103059.035041	43.147316
3509.336668	1102860.130142	43.152321
3509.657339	1102684.940889	43.157325
3509.271547	1102511.295564	43.162330
3509.244439	1102319.621369	43.167335
3509.394728	1102140.524765	43.172340
3508.983485	1101957.023339	43.177345
3509.396796	1101776.915740	43.182349
3508.975148	1101596.748511	43.187354
3508.860580	1101417.193681	43.192359
3508.961999	1101233.296490	43.197364
3508.977592	1101064.603880	43.202369
3509.073462	1100893.694445	43.207373
3508.801143	1100726.759127	43.212378
3509.230729	1100547.181318	43.217383
3509.180935	1100374.176538	43.222388
3508.789549	1100198.545898	43.227393
3509.300286	1100014.444187	43.232397
3509.232798	1099839.130892	43.237402
3509.245518	1099660.070238	43.242407
3509.134988	1099473.088751	43.247412
3508.930292	1099306.098364	43.252417
3508.905722	1099131.519893	43.257421
3508.849457	1098962.104152	43.262426
3509.026780	1098780.979357	43.267431
3508.829069	1098616.165683	43.272436
3508.578334	1098434.526053	43.277441
3508.920601	1098252.782652	43.282445
3508.491095	1098090.094885	43.287450
3508.524402	1097919.101621	43.292455
3508.727977	1097756.108271	43.297460
3508.659596	1097592.294055	43.302465
3508.936026	1097422.297059	43.307469
3508.511119	1097252.314582	43.312474
3508.372629	1097082.183940	43.317479
3508.456186	1096914.880878	43.322484
3508.033498	1096750.047342	43.327489
3508.470098	1096579.136589	43.332493
3508.380240	1096429.543413	43.337498
3508.201728	1096269.342282	43.342503
3508.318613	1096096.364384	43.347508
3508.362826	1095939.273728	43.352513
3508.477270	1095777.192096	43.357517
3507.943599	1095613.011870	43.362522
3508.113819	1095455.408049	43.367527
3508.163455	1095301.550966	43.372532
3508.366602	1095139.531309	43.377537
3508.212631	1094982.062781	43.382541
3508.257024	1094836.804931	43.387546
3508.444922	1094663.865242	43.392551
3508.533335	1094500.984165	43.397556
3507.733481	1094343.603435	43.402561
3508.100830	1094185.356004	43.407565
3508.110817	1094023.526163	43.412570
3508.362427	1093869.212309	43.417575
3508.137967	1093711.239906	43.422580
3508.070623	1093551.418536	43.427585
3508.257916	1093397.388964	43.432589
3508.027782	1093237.872291	43.437594
3508.042191	1093074.577644	43.442599
3508.162682	1092921.981331	43.447604
3507.973363	1092770.963319	43.452609
3507.797591	1092605.962851	43.457613
3507.947174	1092451.816888	43.462618
3507.811566	1092299.245218	43.467623
3507.966505	1092134.367390	43.472628
3507.571428	1091989.871441	43.477633
3507.794618	1091838.376552	43.482637
3507.957857	1091687.748988	43.487642
3507.922124	1091521.256296	43.492647
3507.716331	1091373.936134	43.497652
3507.603681	1091243.831711	43.502657
3507.377221	1091083.006237	43.507661
3507.591658	1090937.903093	43.512666
3507.618310	1090795.316711	43.517671
3507.400397	1090646.733929	43.522676
3507.188795	1090504.945238	43.527681
3507.681271	1090358.631652	43.532685
3507.055708	1090215.275545	43.537690
3507.516835	1090063.787674	43.542695
3507.496732	1089925.304284	43.547700
3507.294991	1089792.785383	43.552705
3507.561263	1089634.900648	43.557709
3507.461796	1089490.385168	43.562714
3507.534990	1089351.871779	43.567719
3507.389519	1089202.471238	43.572724
3507.246340	1089058.430386	43.577729
3507.402110	1088920.754497	43.582733
3507.294257	1088792.218933	43.587738
3507.338461	1088626.965351	43.592743
3507.373471	1088483.167278	43.597748
3507.315985	1088344.074906	43.602753
3507.212072	1088195.502020	43.607757
3507.120690	1088065.892702	43.612762
3507.045304	1087927.750678	43.617767
3507.054660	1087785.854543	43.622772
3507.151297	1087653.042633	43.627777
3507.430635	1087502.183947	43.632781
3507.130049	1087374.508912	43.637786
3507.199821	1087230.384491	43.642791
3507.633417	1087099.994919	43.647796
3507.268853	1086957.372142	43.652801
3507.447394	1086810.056404	43.657805
3507.070638	1086675.765317	43.662810
3507.287401	1086526.806482	43.667815
3507.436153	1086385.042476	43.672820
3507.137564	1086251.398877	43.677825
3507.203421	1086108.299569	43.682829
3507.004795	1085975.974506	43.687834
3507.101460	1085843.118360	43.692839
3507.047619	1085710.283757	43.697844
3506.899157	1085576.215438	43.702849
3507.135878	1085430.386340	43.707853
3507.053707	1085298.600727	43.712858
3506.957814	1085164.705314	43.717863
3506.935277	1085034.820637	43.722868
3506.565552	1084895.116232	43.727873
3506.952570	1084751.544877	43.732877
3506.833620	1084622.816619	43.737882
3506.777148	1084491.678290	43.742887
3506.929888	1084356.955089	43.747892
3506.923005	1084234.430845	43.752897
3506.652008	1084091.046313	43.757901
3506.410324	1083982.744768	43.762906
3506.780392	1083857.657121	43.767911
3506.775862	1083722.081181	43.772916
3506.535210	1083590.951475	43.777921
3506.657064	1083468.676444	43.782925
3506.439090	1083348.660094	43.787930
3506.768910	1083216.180841	43.792935
3506.553855	1083087.815660	43.797940
3506.699514	1082962.840312	43.802945
3506.857911	1082836.229724	43.807949
3506.711445	1082709.282799	43.812954
3506.991760	1082588.016804	43.817959
3506.738847	1082446.024491	43.822964
3506.798327	1082319.130456	43.827969
3507.158063	1082186.141689	43.832973
3506.814472	1082054.608284	43.837978
3506.969422	1081924.716056	43.842983
3507.131102	1081787.242184	43.847988
3506.619562	1081651.410430	43.852993
3506.862725	1081517.081662	43.857997
3506.878067	1081396.216469	43.863002
3507.033320	1081267.171833	43.868007
3506.858809	1081134.629098	43.873012
3506.587837	1081000.372269	43.878017
3506.804924	1080874.473870	43.883021
3506.950132	1080736.112796	43.888026
3506.728219	1080599.823372	43.893031
3506.634565	1080485.767526	43.898036
3506.342412	1080355.144002	43.903041
3506.326846	1080229.748742	43.908045
3506.316115	1080101.279507	43.913050
3506.281931	1079982.501944	43.918055
3506.344366	1079852.767469	43.923060
3506.615137	1079734.509988	43.928065
3506.803255	1079615.208049	43.933069
3506.649283	1079488.187290	43.938074
3506.394236	1079364.154969	43.943079
3507.009847	1079230.476200	43.948084
3506.625484	1079121.141820	43.953089
3506.325498	1078986.360333	43.958093
3506.271306	1078857.005245	43.963098
3506.638159	1078732.856142	43.968103
3506.458154	1078608.314416	43.973108
3506.479685	1078494.101962	43.978113
3506.715397	1078356.337430	43.983117
3506.626303	1078237.338949	43.988122
3506.509271	1078114.215264	43.993127
3506.641933	1077988.648081	43.998132
3506.429872	1077866.878240	44.003137
3506.489617	1077734.022267	44.008141
3505.938952	1077620.845657	44.013146
3506.234312	1077505.895491	44.018151
3506.177387	1077384.281314	44.023156
3506.212369	1077258.521435	44.028161
3506.321900	1077140.522288	44.033165
3506.128439	1077021.322482	44.038170
3506.303245	1076910.411674	44.043175
3506.338744	1076776.672371	44.048180
3506.236133	1076657.545665	44.053185
3506.329294	1076535.887873	44.058189
3506.169191	1076430.591023	44.063194
3506.246330	1076302.785953	44.068199
3506.273203	1076179.498911	44.073204
3506.076078	1076073.049075	44.078209
3506.529343	1075939.988623	44.083213
3506.171139	1075826.359012	44.088218
3506.068188	1075708.075847	44.093223
3505.980048	1075589.595630	44.098228
3505.907308	1075483.113810	44.103233
3505.826026	1075360.786383	44.108237
3505.884533	1075251.397529	44.113242
3505.961300	1075136.913678	44.118247
3506.198266	1075013.277617	44.123252
3505.823460	1074907.794696	44.128257
3506.264580	1074801.310999	44.133261
3505.931568	1074697.930020	44.138266
3505.718777	1074580.216779	44.143271
3505.986103	1074463.574479	44.148276
3505.692455	1074356.818956	44.153281
3505.783126	1074238.279990	44.158285
3505.683710	1074135.906453	44.163290
3505.444552	1074012.998548	44.168295
3505.693334	1073912.676666	44.173300
3505.561027	1073812.703880	44.178305
3505.989978	1073693.905288	44.183309
3505.882489	1073591.330765	44.188314
3505.635411	1073489.257622	44.193319
3505.784205	1073370.978473	44.198324
3505.641756	1073270.997454	44.203329
3505.872080	1073147.608507	44.208333
3505.734694	1073040.609405	44.213338
3505.751112	1072930.220332	44.218343
3505.822052	1072824.239487	44.223348
3505.455456	1072716.791426	44.228353
3505.543104	1072601.195849	44.233357
3505.427241	1072505.423910	44.238362
3505.827246	1072396.786424	44.243367
3505.518898	1072294.316738	44.248372
3505.465085	1072197.760523	44.253377
3505.630463	1072082.813795	44.258381
3505.429446	1071978.014403	44.263386
3505.371888	1071878.954853	44.268391
3505.698384	1071770.797511	44.273396
3505.233239	1071663.825459	44.278401
3505.751280	1071558.226938	44.283405
3505.887309	1071454.707371	44.288410
3505.737540	1071351.425119	44.293415
3506.048910	1071237.397604	44.298420
3505.441919	1071128.131979	44.303425
3505.543894	1071016.344749	44.308429
3505.362162	1070930.743365	44.313434
3505.531490	1070809.810571	44.318439
3505.542254	1070708.315835	44.323444
3505.484370	1070611.059518	44.328449
3505.413692	1070506.691054	44.333453
3505.610478	1070390.934715	44.338458
3505.611709	1070291.452288	44.343463
3505.686503	1070180.613670	44.348468
3505.450206	1070083.473490	44.353473
3505.548688	1069967.820526	44.358477
3505.768202	1069869.640236	44.363482
3505.411064	1069768.477057	44.368487
3505.597374	1069662.704390	44.373492
3505.510325	1069561.877433	44.378497
3505.644239	1069447.168964	44.383501
3505.464983	1069351.929092	44.388506
3505.335259	1069247.065674	44.393511
3505.539812	1069135.896140	44.398516
3505.328682	1069048.058961	44.403521
3505.505589	1068942.466228	44.408525
3505.339229	1068842.408235	44.413530
3504.995522	1068748.050250	44.418535
3505.287952	1068640.798196	44.423540
3504.989391	1068550.659888	44.428545
3505.538697	1068439.227151	44.433549
3505.552819	1068341.149466	44.438554
3505.217363	1068251.300771	44.443559
3505.019625	1068145.465927	44.448564
3505.137727	1068051.116039	44.453569
3505.060379	1067955.546638	44.458573
3505.093628	1067871.015945	44.463578
3505.094762	1067766.775783	44.468583
3505.303732	1067666.249851	44.473588
3504.983003	1067566.193984	44.478593
3505.211066	1067469.123303	44.483597
3505.242323	1067374.199064	44.488602
3505.170929	1067280.732668	44.493607
3505.159509	1067180.137955	44.498612
3504.892186	1067093.048086	44.503617
3505.009686	1066981.945401	44.508621
3504.949211	1066906.936815	44.513626
3504.888186	1066810.190624	44.518631
3505.282099	1066709.135798	44.523636
3504.848711	1066623.412368	44.528641
3505.021728	1066541.050379	44.533645
3504.890976	1066442.000743	44.538650
3504.782973	1066340.540863	44.543655
3504.964349	1066253.363761	44.548660
3504.934666	1066161.795228	44.553665
3505.256343	1066074.015023	44.558669
3505.174891	1065976.487954	44.563674
3504.799988	1065878.045517	44.568679
3505.010288	1065783.352858	44.573684
3504.657909	1065701.160998	44.578689
3504.649278	1065599.286249	44.583693
3504.924727	1065509.580609	44.588698
3504.599824	1065431.228295	44.593703
3504.725272	1065334.906406	44.598708
3504.588579	1065255.654734	44.603713
3504.771604	1065161.725508	44.608717
3504.899545	1065088.777636	44.613722
3504.862902	1064997.287034	44.618727
3504.846253	1064907.234818	44.623732
3504.794485	1064821.324155	44.628737
3504.822889	1064732.031366	44.633741
3504.738430	1064639.388077	44.638746
3504.764703	1064548.745605	44.643751
3504.844258	1064457.515533	44.648756
3504.984920	1064369.545462	44.653761
3505.027021	1064272.256436	44.658765
3504.990069	1064197.591845	44.663770
3504.554553	1064103.650174	44.668775
3504.577072	1064009.535229	44.673780
3504.563760	1063929.474261	44.678785
3504.728535	1063837.353780	44.683789
3504.854914	1063749.761069	44.688794
3504.841680	1063672.198417	44.693799
3504.794843	1063577.510085	44.698804
3504.645240	1063483.799430	44.703809
3504.679284	1063400.354608	44.708813
3504.780873	1063322.190665	44.713818
3504.521306	1063231.862267	44.718823
3504.609065	1063152.735764	44.723828
3504.448123	1063068.355572	44.728833
3504.824698	1062985.714253	44.733837
3504.445273	1062896.747545	44.738842
3504.641440	1062816.924614	44.743847
3504.878522	1062725.158588	44.748852
3504.646750	1062641.457269	44.753857
3504.884586	1062539.388921	44.758861
3504.667346	1062457.222481	44.763866
3504.369960	1062381.998572	44.768871
3504.488504	1062295.154035	44.773876
3504.422319	1062220.948695	44.778881
3504.392465	1062134.222318	44.783885
3504.285066	1062061.946861	44.788890
3504.431770	1061980.194666	44.793895
3504.721338	1061897.551332	44.798900
3504.248046	1061823.889013	44.803905
3504.250495	1061738.595088	44.808909
3504.626585	1061657.666743	44.813914
3504.458993	1061568.643642	44.818919
3504.740081	1061486.091797	44.823924
3504.237471	1061402.223665	44.828929
3504.305032	1061312.483764	44.833933
3504.399429	1061254.702183	44.838938
3504.307813	1061180.101876	44.843943
3504.409823	1061089.197315	44.848948
3504.162602	1061025.307643	44.853953
3504.435807	1060943.904342	44.858957
3504.404406	1060853.306705	44.863962
3504.464029	1060773.958041	44.868967
3504.418136	1060686.344903	44.873972
3504.306777	1060608.947767	44.878977
3504.221303	1060532.893340	44.883981
3504.116847	1060447.982172	44.888986
3504.167968	1060384.132207	44.893991
3504.391507	1060298.490664	44.898996
3503.764663	1060225.891450	44.904001
3504.064150	1060149.479436	44.909005
3504.355951	1060078.171426	44.914010
3504.131502	1060009.547597	44.919015
3504.118839	1059929.813472	44.924020
3504.032703	1059867.520930	44.929025
3504.194518	1059783.807582	44.934029
3504.014765	1059699.475085	44.939034
3504.078145	1059639.948177	44.944039
3504.143678	1059553.935855	44.949044
3504.015267	1059484.711821	44.954049
3504.073535	1059399.565060	44.959053
3503.961319	1059331.973705	44.964058
3504.061812	1059275.422387	44.969063
3504.276452	1059199.011164	44.974068
3504.332340	1059125.321839	44.979073
3503.927314	1059043.424258	44.984077
3504.292952	1058974.401387	44.989082
3504.331282	1058893.295410	44.994087
3504.439183	1058819.304468	44.999092
3504.036155	1058753.680311	45.004097
3504.060006	1058659.184608	45.009101
3504.351562	1058589.880155	45.014106
3504.176261	1058513.523647	45.019111
3504.237149	1058436.838200	45.024116
3504.166434	1058370.480455	45.029121
3503.996652	1058288.051250	45.034125
3504.232937	1058232.815476	45.039130
3504.043667	1058157.997623	45.044135
3504.195101	1058069.732349	45.049140
3503.884375	1058006.877744	45.054145
3503.938517	1057923.731868	45.059149
3503.891270	1057851.583860	45.064154
3503.804848	1057785.799680	45.069159
3503.953205	1057719.205332	45.074164
3504.071744	1057649.050494	45.079169
3504.265181	1057564.527490	45.084173
3504.109475	1057502.315988	45.089178
3503.838211	1057431.355490	45.094183
3504.083090	1057359.827343	45.099188
3503.673334	1057291.970915	45.104193
3503.716977	1057223.749933	45.109197
3503.654180	1057148.993892	45.114202
3503.802247	1057098.867796	45.119207
3503.691351	1057026.334066	45.124212
3503.707106	1056956.861806	45.129217
3504.238554	1056890.772475	45.134221
3503.911419	1056825.305534	45.139226
3503.502842	1056752.720874	45.144231
3503.871485	1056691.570133	45.149236
3503.660999	1056625.021670	45.154241
3503.877859	1056548.187896	45.159245
3503.872751	1056477.942160	45.164250
3503.468649	1056416.241109	45.169255
3503.650006	1056356.562932	45.174260
3503.476495	1056290.582519	45.179265
3503.797494	1056222.785293	45.184269
3503.690605	1056152.359441	45.189274
3503.393851	1056093.528095	45.194279
3504.021313	1056024.907025	45.199284
3503.845984	1055962.006782	45.204289
3503.808735	1055881.254399	45.209293
3504.019799	1055824.649461	45.214298
3503.801525	1055766.958173	45.219303
3503.928591	1055706.125422	45.224308
3503.934355	1055620.061533	45.229313
3504.128726	1055546.879805	45.234317
3503.908549	1055488.800410	45.239322
3503.573446	1055427.558814	45.244327
3503.973610	1055354.629781	45.249332
3503.636201	1055300.808458	45.254337
3503.718496	1055233.231155	45.259341
3503.867701	1055163.714326	45.264346
3503.500128	1055089.848015	45.269351
3503.618838	1055032.189922	45.274356
3503.739000	1054971.350209	45.279361
3503.566423	1054908.533882	45.284365
3504.063777	1054846.666788	45.289370
3503.346095	1054774.010580	45.294375
3504.060597	1054710.563947	45.299380
3503.697858	1054643.438285	45.304385
3503.856120	1054567.068542	45.309389
3503.894386	1054500.453462	45.314394
3503.493043	1054449.622617	45.319399
3503.677428	1054376.523413	45.324404
3503.514869	1054320.446573	45.329409
3503.619549	1054253.624778	45.334413
3503.897235	1054180.796816	45.339418
3503.435450	1054121.778803	45.344423
3503.389570	1054069.150668	45.349428
3503.353272	1053994.154685	45.354433
3503.681282	1053938.957216	45.359437
3503.904779	1053882.812347	45.364442
3503.737623	1053819.307881	45.369447
3503.728252	1053744.400478	45.374452
3503.763344	1053690.116445	45.379457
3503.520216	1053625.272522	45.384461
3503.512183	1053557.496758	45.389466
3503.581632	1053494.335232	45.394471
3503.885102	1053434.123280	45.399476
3503.490416	1053379.424905	45.404481
3503.376629	1053309.638799	45.409485
3503.684584	1053248.845591	45.414490
3503.583983	1053204.220860	45.419495
3503.940127	1053124.713197	45.424500
3503.547269	1053063.647695	45.429505
3503.559772	1052999.429261	45.434509
3503.813428	1052942.402073	45.439514
3503.724963	1052877.427468	45.444519
3503.707785	1052806.172729	45.449524
3503.566338	1052746.894393	45.454529
3503.431929	1052694.942721	45.459533
3503.708398	1052620.358702	45.464538
3503.467626	1052556.851834	45.469543
3503.376968	1052499.780357	45.474548
3503.406929	1052434.298881	45.479553
3503.523227	1052379.313569	45.484557
3503.531652	1052327.817082	45.489562
3503.380197	1052270.946120	45.494567
3503.487251	1052198.891611	45.499572
3503.292458	1052152.730922	45.504577
3503.527275	1052092.515663	45.509581
3503.544922	1052033.589217	45.514586
3503.308725	1051963.806262	45.519591
3503.381852	1051911.427280	45.524596
3503.090957	1051855.828737	45.529601
3503.504167	1051790.276510	45.534605
3503.662992	1051734.313349	45.539610
3503.272983	1051677.764899	45.544615
3503.569823	1051608.950565	45.549620
3503.281358	1051559.810520	45.554625
3503.236580	1051496.355623	45.559629
3503.256883	1051446.488581	45.564634
3503.021869	1051394.541245	45.569639
3503.219444	1051332.201944	45.574644
3503.478458	1051282.101203	45.579649
3503.227365	1051223.113925	45.584653
3503.302361	1051171.499245	45.589658
3502.827326	1051123.736397	45.594663
3503.281568	1051062.412783	45.599668
3503.358506	1051019.959638	45.604673
3503.171886	1050959.126251	45.609677
3503.094258	1050909.463409	45.614682
3503.164554	1050852.541321	45.619687
3502.929442	1050793.546823	45.624692
3503.102556	1050747.989021	45.629697
3502.996152	1050689.261595	45.634701
3502.940036	1050642.004357	45.639706
3502.813500	1050599.388568	45.644711
3503.064182	1050558.639611	45.649716
3503.057317	1050498.253868	45.654721
3502.849698	1050443.399113	45.659725
3502.851267	1050404.908778	45.664730
3502.845041	1050364.490104	45.669735
3503.201089	1050308.672969	45.674740
3502.895029	1050260.681887	45.679745
3502.967604	1050210.119797	45.684749
3502.850520	1050166.920294	45.689754
3502.513594	1050121.537807	45.694759
3502.902491	1050056.837295	45.699764
3502.825984	1050021.830182	45.704769
3502.492708	1049974.516412	45.709773
3502.501951	1049928.978855	45.714778
3502.799100	1049884.551219	45.719783
3503.273414	1049844.821413	45.724788
3502.741346	1049799.082509	45.729793
3502.706758	1049747.665544	45.734797
3503.037810	1049701.590722	45.739802
3502.855809	1049662.546578	45.744807
3503.018319	1049612.446614	45.749812
3502.856247	1049552.365546	45.754817
3502.701542	1049492.572062	45.759821
3503.098819	1049391.295242	45.764826
3502.841691	1049222.390442	45.769831
3502.929790	1048990.318422	45.774836
3502.607431	1048698.476594	45.779841
3502.796085	1048345.449190	45.784845
3502.945871	1047928.323274	45.789850
3502.439689	1047462.628948	45.794855
3502.419097	1046922.586140	45.799860
3502.253637	1046306.346203	45.804865
3502.197714	1045646.475811	45.809869
3502.400690	1044903.440726	45.814874
3501.725655	1044112.355683	45.819879
3502.056623	1043224.787141	45.824884
3501.697744	1042283.089725	45.829889
3501.449818	1041263.237384	45.834893
3501.706893	1040173.627064	45.839898
3501.311042	1039017.791906	45.844903
3501.492264	1037769.672740	45.849908
3501.158135	1036461.785488	45.854913
3501.011010	1035057.987536	45.859917
3500.684529	1033575.974088	45.864922
3499.939610	1032029.659744	45.869927
3500.496013	1030403.798640	45.874932
3499.773608	1028693.226714	45.879937
3499.527732	1026885.371021	45.884941
3499.800849	1025004.842598	45.889946
3499.142746	1023045.797400	45.894951
3498.780102	1021000.193424	45.899956
3498.655748	1018877.453720	45.904961
3498.378526	1016670.083197	45.909965
3498.185568	1014378.235424	45.914970
3497.336620	1012007.272657	45.919975
3497.247113	1009549.574943	45.924980
3496.959099	1007016.562985	45.929985
3496.399207	1004395.796593	45.934989
3495.983538	1001689.325109	45.939994
3495.562840	998906.788116	45.944999
3495.028943	996036.794315	45.950004
3494.720503	993090.462844	45.955009
3494.342106	990058.852885	45.960013
3494.098686	986933.309179	45.965018
3493.453444	983733.487794	45.970023
3492.919388	980438.182470	45.975028
3492.362511	977079.407954	45.980033
3491.980601	973637.074524	45.985037
3491.511776	970094.640000	45.990042
3490.408579	966486.675224	45.995047
3490.231944	962798.891938	46.000052
3489.667769	959030.966649	46.005057
3488.956888	955170.837367	46.010061
3488.300222	951302.867569	46.015066
3487.774476	947397.477185	46.020071
3487.123480	943393.222597	46.025076
3486.415981	939318.372880	46.030081
3485.959619	935140.681316	46.035085
3485.152870	930884.526026	46.040090
3483.978127	926559.941829	46.045095
3483.357954	922149.131311	46.050100
3482.677859	917659.528830	46.055105
3481.802053	913091.575035	46.060109
3480.726427	908433.536962	46.065114
3479.854536	903718.658034	46.070119
3479.028521	898908.889077	46.075124
3478.189011	894027.828164	46.080129
3477.581881	889059.906312	46.085133
3476.552724	883993.427678	46.090138
3475.397712	878859.547334	46.095143
3474.659193	873647.180441	46.100148
3473.847776	868354.504473	46.105153
3472.602742	862978.309234	46.110157
3471.431422	857509.879766	46.115162
3470.460510	851962.835868	46.120167
3469.522181	846345.340331	46.125172
3468.383861	840645.695039	46.130177
3467.484316	834869.432603	46.135181
3466.711205	828996.542457	46.140186
3465.303770	823050.583267	46.145191
3464.573389	817011.336318	46.150196
3463.569619	810909.700354	46.155201
3462.327721	804699.474041	46.160205
3461.237185	798398.345349	46.165210
3459.734463	792039.999204	46.170215
3458.858149	785577.768922	46.175220
3457.365266	779039.970205	46.180225
3456.073138	772429.902241	46.185229
3454.741697	765729.997360	46.190234
3453.534275	758968.217158	46.195239
3452.441136	752108.335089	46.200244
3451.320774	745182.452930	46.205249
3449.686323	738155.641444	46.210253
3448.568332	731039.162249	46.215258
3446.976181	723858.337739	46.220263
3445.687747	716579.244780	46.225268
3444.368853	709227.028662	46.230273
3442.798912	701786.746327	46.235277
3441.609170	694267.842716	46.240282
3439.565177	686683.841755	46.245287
3438.497427	678990.507319	46.250292
3436.974737	671245.388084	46.255297
3435.520436	663418.858496	46.260301
3433.999252	655496.745120	46.265306
3432.106000	647499.957452	46.270311
3430.614504	639421.231974	46.275316
3428.999796	631287.901087	46.280321
3427.318708	623059.593643	46.285325
3425.638661	614756.948357	46.290330
3423.460647	606382.147737	46.295335
3422.086145	597928.502093	46.300340
3420.472329	589407.184768	46.305345
3418.453187	580799.791037	46.310349
3416.596339	572121.268092	46.315354
3414.545127	563387.720520	46.320359
3412.807896	554558.868892	46.325364
3410.820262	545672.118560	46.330369
3409.303818	536712.642375	46.335373
3407.084369	527669.833153	46.340378
3404.751722	518576.776929	46.345383
3403.068646	509387.760463	46.350388
3400.527268	500139.737378	46.355393
3398.728156	490832.803774	46.360397
3396.888704	481449.430613	46.365402
3394.445075	472008.243020	46.370407
3392.227825	462487.946615	46.375412
3389.696872	452922.099949	46.380417
3387.478985	443273.372899	46.385421
3385.247498	433573.705649	46.390426
3382.632297	423812.308019	46.395431
3380.223335	413980.455782	46.400436
3378.201902	404101.267438	46.405441
3375.161887	394159.078826	46.410445
3372.787228	384161.928249	46.415450
3369.973893	374113.779693	46.420455
3367.266798	364016.556285	46.425460
3365.088531	353863.967155	46.430465
3362.332786	343666.947411	46.435469
3359.022095	333405.185766	46.440474
3356.086888	323111.696796	46.445479
3353.347194	312771.816990	46.450484
3350.566418	302389.884861	46.455489
3347.146994	291960.681053	46.460493
3344.311655	281508.665725	46.465498
3340.813676	270989.775570	46.470503
3337.505404	260469.523573	46.475508
3334.499811	249898.283913	46.480513
3330.525445	239293.619670	46.485517
3327.410919	228630.874907	46.490522
3323.720527	217933.740193	46.495527
3320.203018	207261.034926	46.500532
3316.232162	196579.154953	46.505537
3312.202167	185885.971524	46.510541
3308.141386	175164.610579	46.515546
3303.692022	164461.446806	46.520551
3299.256450	153752.732764	46.525556
3294.585083	143028.609113	46.530561
3289.479119	132339.181823	46.535565
3284.759685	121660.879549	46.540570
3279.307629	111017.926053	46.545575
3273.820825	100395.101415	46.550580
3267.719228	89823.814107	46.555585
3260.376652	79296.186070	46.560589
3253.068273	68849.220966	46.565594
3244.123676	58512.072230	46.570599
3233.061265	48341.837816	46.575604
3209.953224	38638.455734	46.580609
3170.489220	29666.156126	46.585613
3119.766988	21478.183513	46.590618
3064.078929	14201.104250	46.595623
3010.996757	7846.753767	46.600628
2961.010822	2500.674134	46.605633
2836.138960	407.182215	46.610637
2700.629817	396.728892	46.615642
2651.023675	405.000518	46.620647
2672.949273	393.675928	46.625652
2732.365412	382.089512	46.630657
2795.284553	370.758020	46.635661
2842.020841	363.285245	46.640666
2866.036037	370.783508	46.645671
2871.296973	368.650670	46.650676
2865.312659	378.222007	46.655681
2855.182904	371.593084	46.660685
2846.419110	354.001589	46.665690
2839.933891	359.720712	46.670695
2835.862155	360.402645	46.675700
2833.724980	356.661658	46.680705
2831.794643	362.973421	46.685709
2830.397637	356.835742	46.690714
2828.973104	346.777576	46.695719
2826.911167	343.995681	46.700724
2824.051569	331.769999	46.705729
2820.914376	351.362130	46.710733
2817.565630	344.466994	46.715738
2814.508758	341.108694	46.720743
2811.419630	332.611175	46.725748
2808.403550	340.192102	46.730753
2805.117673	343.127884	46.735757
2802.331833	332.677150	46.740762
2799.097060	342.951991	46.745767
2795.966319	331.130732	46.750772
2793.038626	325.173504	46.755777
2789.289264	328.215298	46.760781
2786.652212	328.313158	46.765786
2783.167418	330.172624	46.770791
2779.574797	328.237711	46.775796
2776.321176	331.273255	46.780801
2773.714854	325.350662	46.785805
2770.416490	324.879772	46.790810
2766.762428	327.087987	46.795815
2763.353503	314.238825	46.800820
2760.190471	326.244833	46.805825
2756.364991	322.183466	46.810829
2753.470559	322.274442	46.815834
2749.997533	317.441278	46.820839
2746.602739	319.837419	46.825844
2743.223008	315.089411	46.830849
2739.854786	324.978209	46.835853
2736.951399	314.334488	46.840858
2733.489199	318.066332	46.845863
2730.306341	307.602178	46.850868
2726.630916	310.540548	46.855873
2722.903982	321.981879	46.860877
2720.066808	310.271610	46.865882
2716.225180	313.866924	46.870887
2712.619258	307.031623	46.875892
2709.356454	307.189367	46.880897
2706.019590	313.155091	46.885901
2702.856469	303.509425	46.890906
2699.151987	305.004790	46.895911
2695.641018	298.928905	46.900916
2692.558747	304.686317	46.905921
2689.022910	308.067454	46.910925
2685.646715	299.821271	46.915930
2682.512619	299.782293	46.920935
2678.851359	300.983841	46.925940
2675.203901	289.491855	46.930945
2671.244627	299.526551	46.935949
2668.349324	300.768548	46.940954
2665.359600	301.023452	46.945959
2661.638774	299.817117	46.950964
2658.216954	296.353322	46.955969
2654.148360	300.207373	46.960973
2651.446899	285.644876	46.965978
2647.748459	302.533652	46.970983
2644.187878	286.560525	46.975988
2640.810041	287.842825	46.980993
2637.062674	298.688981	46.985997
2633.699579	290.644005	46.991002
2630.228670	291.405549	46.996007
2626.456736	293.217513	47.001012
2623.334478	282.387484	47.006017
2619.800471	294.663830	47.011021
2616.661254	294.929491	47.016026
2613.265962	293.378662	47.021031
2610.204500	285.351744	47.026036
2607.094023	284.655788	47.031041
2602.914925	284.473049	47.036045
2599.406873	288.009069	47.041050
2595.712224	285.099070	47.046055
2591.882658	284.087989	47.051060
2588.417440	287.597416	47.056065
2584.945205	291.936729	47.061069
2582.021935	286.756304	47.066074
2578.816017	279.199453	47.071079
2575.304994	283.851298	47.076084
2571.889035	279.527273	47.081089
2568.030897	291.061206	47.086093
2564.589858	287.464085	47.091098
2560.972466	282.224980	47.096103
2557.565503	283.636525	47.101108
2554.167582	285.552202	47.106113
2550.482814	279.864567	47.111117
2547.304411	273.998828	47.116122
2543.826816	290.025441	47.121127
2540.480116	281.930755	47.126132
2536.922904	276.216472	47.131137
2533.015820	285.295200	47.136141
2529.771604	280.740233	47.141146
2525.903346	281.246509	47.146151
2522.959784	286.694499	47.151156
2519.440812	276.891168	47.156161
2515.877441	276.643942	47.161165
2512.358896	277.824400	47.166170
2508.792834	274.882097	47.171175
2505.407539	277.389532	47.176180
2502.084446	268.927229	47.181185
2498.304169	273.188521	47.186189
2494.996691	265.578517	47.191194
2491.757334	276.210221	47.196199
2488.484742	268.692829	47.201204
2484.969153	265.918123	47.206209
2480.887546	276.188819	47.211213
2477.250856	257.119974	47.216218
2474.196831	267.970522	47.221223
2470.243870	268.579190	47.226228
2466.994544	264.554202	47.231233
2463.010812	272.940387	47.236237
2460.285507	273.895745	47.241242
2456.642467	266.993222	47.246247
2453.607590	261.653782	47.251252
2450.090288	265.208453	47.256257
2445.775464	269.685382	47.261261
2442.761972	264.142638	47.266266
2439.012016	270.366186	47.271271
2435.718081	260.660963	47.276276
2432.522122	253.262579	47.281281
2428.729006	262.620489	47.286285
2425.255114	249.808240	47.291290
2421.756073	264.986887	47.296295
2418.099281	262.860495	47.301300
2414.891192	258.165064	47.306305
2411.175547	276.123799	47.311309
2407.654985	267.736337	47.316314
2404.330688	259.480780	47.321319
2400.791858	272.645696	47.326324
2397.712584	257.975871	47.331329
2394.110221	256.413124	47.336333
2390.573464	261.216577	47.341338
2386.686635	263.523622	47.346343
2382.815761	258.389466	47.351348
2379.832901	260.051585	47.356353
2376.140006	263.619459	47.361357
2372.920590	253.504298	47.366362
2369.450779	265.149364	47.371367
2365.783723	263.253774	47.376372
2362.516604	246.043059	47.381377
2359.044093	260.528914	47.386381
2355.662084	253.189467	47.391386
2351.965805	249.475025	47.396391
2348.591835	258.583593	47.401396
2345.108116	256.656003	47.406401
2341.141933	250.836631	47.411405
2337.820015	258.085215	47.416410
2334.356345	262.129014	47.421415
2330.706564	246.755286	47.426420
2327.421076	248.981930	47.431425
2323.802778	253.181163	47.436429
2320.680943	242.126117	47.441434
2317.074507	247.097263	47.446439
2313.312809	254.064008	47.451444
2310.026056	250.161192	47.456449
2306.522028	245.823322	47.461453
2302.927013	247.180749	47.466458
2299.286638	239.780359	47.471463
2295.604742	252.958924	47.476468
2292.849914	251.516706	47.481473
2289.277724	252.294710	47.486477
2285.695722	245.448524	47.491482
2281.809315	252.004618	47.496487
2278.827321	253.554952	47.501492
2275.523669	254.709151	47.506497
2271.534878	255.559622	47.511501
2268.086583	243.171028	47.516506
2264.256794	246.277713	47.521511
2260.831116	252.213932	47.526516
2257.489658	245.295630	47.531521
2253.585132	253.141610	47.536525
2250.636162	245.574331	47.541530
2247.647479	253.716870	47.546535
2243.611864	250.785655	47.551540
2239.909907	243.456818	47.556545
2236.271005	247.412055	47.561549
2232.784772	236.165289	47.566554
2229.424399	239.069174	47.571559
2226.107229	248.660809	47.576564
2222.540503	247.774386	47.581569
2219.203845	237.934966	47.586573
2216.149023	241.802064	47.591578
2212.165448	244.266032	47.596583
2208.454479	248.293250	47.601588
2205.062778	237.720916	47.606593
2201.319828	249.051374	47.611597
2197.953030	241.334906	47.616602
2194.550865	245.042158	47.621607
2190.920321	242.762979	47.626612
2187.678812	242.431745	47.631617
2184.040702	248.580910	47.636621
2180.519481	240.096424	47.641626
2177.426523	236.084463	47.646631
2173.867013	242.420347	47.651636
2170.294291	234.237278	47.656641
2166.130799	241.833190	47.661645
2163.277200	234.695763	47.666650
2159.779772	239.473385	47.671655
2155.904646	241.212319	47.676660
2152.915710	234.294534	47.681665
2148.928242	231.661667	47.686669
2145.380961	238.818935	47.691674
2142.334333	228.124514	47.696679
2138.403816	229.286373	47.701684
2135.445927	232.071916	47.706689
2131.431811	240.358765	47.711693
2127.836790	236.681610	47.716698
2124.582969	229.713315	47.721703
2121.087685	230.719830	47.726708
2117.895472	233.828854	47.731713
2114.138560	228.004309	47.736717
2110.713452	229.779827	47.741722
2106.962860	232.721885	47.746727
2103.134158	230.502077	47.751732
2100.215184	220.112984	47.756737
2096.519487	245.334864	47.761741
2093.531821	224.501731	47.766746
2089.873696	232.192785	47.771751
2085.993691	229.762331	47.776756
2082.486411	231.511362	47.781761
2078.929117	231.194185	47.786765
2075.858520	228.973647	47.791770
2072.270193	233.560894	47.796775
2068.681206	238.565967	47.801780
2065.067903	231.092485	47.806785
2061.595501	231.106120	47.811789
2057.925671	229.732749	47.816794
2054.730301	224.699772	47.821799
2050.979784	234.448873	47.826804
2047.645282	219.147955	47.831809
2044.056301	238.447525	47.836813
2040.603180	221.244143	47.841818
2037.110561	236.160675	47.846823
2033.417465	226.611613	47.851828
2030.067579	227.252044	47.856833
2026.356556	229.831659	47.861837
2023.134070	227.804509	47.866842
2020.080543	239.971663	47.871847
2016.465612	232.916190	47.876852
2012.658566	225.929411	47.881857
2008.647116	220.420691	47.886861
2005.573821	225.620409	47.891866
2002.120271	227.373734	47.896871
1998.378897	226.165213	47.901876
1995.063259	224.465987	47.906881
1991.474735	229.887642	47.911885
1988.277866	232.492855	47.916890
1984.813416	224.363957	47.921895
1981.002136	228.693730	47.926900
1977.418313	223.562682	47.931905
1974.095765	234.517338	47.936909
1970.929232	221.726702	47.941914
1967.260557	219.493000	47.946919
1963.717592	220.485552	47.951924
1959.884713	219.714990	47.956929
1956.424056	230.045738	47.961933
1953.145225	228.847457	47.966938
1949.897633	223.209009	47.971943
1946.039018	233.005976	47.976948
1942.665628	219.703517	47.981953
1939.102142	236.210081	47.986957
1935.594296	224.493909	47.991962
1932.071188	223.192194	47.996967
1928.608254	232.057882	48.001972
1925.296748	219.479034	48.006977
1921.668903	222.623006	48.011981
1918.059171	227.163832	48.016986
1914.621416	221.431776	48.021991
1910.793743	230.474947	48.026996
1907.726199	225.974220	48.032001
1904.195234	220.567725	48.037005
1900.578293	217.878017	48.042010
1897.209365	225.216490	48.047015
1893.931590	226.751444	48.052020
1890.021588	220.201707	48.057025
1886.319018	224.108801	48.062029
1883.238041	220.576449	48.067034
1879.484368	229.631495	48.072039
1875.951482	220.961769	48.077044
1872.713480	221.975282	48.082049
1869.150252	230.971290	48.087053
1865.286700	228.226095	48.092058
1861.942571	221.526387	48.097063
1858.689224	234.202075	48.102068
1855.487524	218.827670	48.107073
1851.489517	226.038993	48.112077
1847.871542	229.889036	48.117082
1844.513549	222.576303	48.122087
1841.160553	220.993316	48.127092
1837.869081	224.223600	48.132097
1833.865488	240.839810	48.137101
1830.265558	217.426972	48.142106
1827.064598	223.936174	48.147111
1823.619820	220.059577	48.152116
1820.672407	219.476260	48.157121
1816.636577	232.647471	48.162125
1813.016327	217.107743	48.167130
1809.414601	207.597325	48.172135
1805.723249	224.497838	48.177140
1802.790551	217.016797	48.182145
1798.689622	215.137944	48.187149
1795.322204	222.088978	48.192154
1792.042695	214.932820	48.197159
1788.588546	219.118322	48.202164
1785.544923	214.664419	48.207169
1781.860336	215.615509	48.212173
1778.264331	211.484988	48.217178
1774.705993	218.554249	48.222183
1770.941021	209.683641	48.227188
1767.639632	211.888181	48.232193
1763.515289	219.525767	48.237197
1760.495683	214.127816	48.242202
1757.508970	217.040786	48.247207
1753.520365	220.677955	48.252212
1749.842430	205.999894	48.257217
1746.413535	214.957993	48.262221
1742.865173	214.918509	48.267226
1739.562892	203.622276	48.272231
1735.860219	209.498635	48.277236
1732.639795	204.689962	48.282241
1728.832158	208.438657	48.287245
1725.572361	207.923301	48.292250
1722.139579	207.831806	48.297255
1717.835522	208.880504	48.302260
1714.673184	201.881063	48.307265
1711.103843	215.038373	48.312269
1708.440625	207.646696	48.317274
1704.908226	211.995793	48.322279
1700.857170	218.563326	48.327284
1697.538716	208.439748	48.332289
1693.973344	209.594174	48.337293
1690.689908	208.662064	48.342298
1687.282416	205.552856	48.347303
1683.081035	211.523172	48.352308
1679.752249	200.667410	48.357313
1676.300533	195.882037	48.362317
1672.996820	207.400252	48.367322
1669.728242	205.194119	48.372327
1665.901152	210.134272	48.377332
1662.841606	199.671634	48.382337
1659.039339	206.313657	48.387341
1655.383393	208.932506	48.392346
1651.896714	201.129195	48.397351
1648.245192	212.494086	48.402356
1645.018736	201.087530	48.407361
1641.221148	202.036421	48.412365
1637.810296	205.870926	48.417370
1634.195849	200.162366	48.422375
1630.742110	199.138422	48.427380
1627.876166	201.779443	48.432385
1623.919920	209.726563	48.437389
1620.514894	192.180519	48.442394
1617.141119	200.993911	48.447399
1613.597361	211.877249	48.452404
1610.039208	200.940003	48.457409
1606.422818	207.943142	48.462413
1603.065623	212.180008	48.467418
1599.644297	199.911712	48.472423
1595.686044	211.142751	48.477428
1592.293183	190.728559	48.482433
1588.738316	213.241751	48.487437
1585.138047	214.670925	48.492442
1581.830372	203.808084	48.497447
1578.348383	209.006931	48.502452
1575.000794	205.924201	48.507457
1571.336999	196.738496	48.512461
1568.065252	210.434734	48.517466
1564.383945	205.970942	48.522471
1560.823201	203.440353	48.527476
1557.929229	202.228768	48.532481
1554.132338	212.092164	48.537485
1550.554457	197.028958	48.542490
1547.020522	199.297323	48.547495
1543.301409	210.694125	48.552500
1539.894225	196.524305	48.557505
1535.970409	202.055153	48.562509
1532.448833	202.378946	48.567514
1529.338469	201.187200	48.572519
1525.593338	200.649627	48.577524
1522.560194	190.366511	48.582529
1518.922234	200.193526	48.587533
1515.439757	206.476020	48.592538
1511.749810	203.326205	48.597543
1508.617035	202.069700	48.602548
1505.132420	204.632327	48.607553
1501.455762	203.317303	48.612557
1497.583661	198.939298	48.617562
1494.426492	192.837683	48.622567
1490.731130	208.094745	48.627572
1487.367521	196.042525	48.632577
1483.685998	213.729774	48.637581
1480.055994	197.012960	48.642586
1476.872269	195.083757	48.647591
1473.185060	205.540553	48.652596
1469.734077	197.842644	48.657601
1466.460444	192.723541	48.662605
1462.626271	200.742139	48.667610
1459.496680	200.216271	48.672615
1455.525105	205.813742	48.677620
1452.132508	191.952538	48.682625
1448.773526	191.306191	48.687629
1445.741924	201.614049	48.692634
1442.235647	191.620483	48.697639
1438.543056	199.647689	48.702644
1434.847755	197.825232	48.707649
1430.959460	205.243874	48.712653
1427.666076	198.260294	48.717658
1424.503817	195.023340	48.722663
1420.611554	198.691838	48.727668
1417.384293	197.563141	48.732673
1413.772544	197.679703	48.737677
1410.183492	204.060236	48.742682
1406.900927	198.708033	48.747687
1402.841944	204.729280	48.752692
1399.430684	190.577789	48.757697
1396.308372	198.525984	48.762701
1392.948656	201.809154	48.767706
1389.589810	197.862869	48.772711
1386.035638	202.086067	48.777716
1382.376394	198.630259	48.782721
1378.854145	190.522118	48.787725
1374.948858	185.228520	48.792730
1371.426251	199.237026	48.797735
1367.786714	188.288413	48.802740
1364.774010	191.310200	48.807745
1360.970774	186.086780	48.812749
1358.086504	188.555319	48.817754
1354.165605	189.145087	48.822759
1350.463820	193.753448	48.827764
1347.091657	186.847046	48.832769
1343.671225	188.873615	48.837773
1340.320378	183.823560	48.842778
1337.148739	193.083456	48.847783
1333.323196	198.006149	48.852788
1329.743766	181.747850	48.857793
1326.079509	180.485433	48.862797
1322.503485	197.350472	48.867802
1319.173236	188.552938	48.872807
1315.621956	182.272890	48.877812
1312.343257	179.062614	48.882817
1308.715116	190.234443	48.887821
1305.264118	181.272070	48.892826
1301.917932	180.591127	48.897831
1297.784863	187.321556	48.902836
1294.619777	186.976736	48.907841
1290.993858	186.299450	48.912845
1287.422265	188.439392	48.917850
1284.174629	180.865390	48.922855
1280.867664	188.325271	48.927860
1277.454776	188.312595	48.932865
1273.621361	189.923754	48.937869
1269.973828	182.324610	48.942874
1266.769001	184.139624	48.947879
1262.933721	182.477601	48.952884
1259.255391	178.864604	48.957889
1255.972198	183.332486	48.962893
1252.687755	190.994556	48.967898
1249.277142	183.430111	48.972903
1245.828728	180.412836	48.977908
1242.303963	189.699977	48.982913
1238.583861	184.548443	48.987917
1234.827304	191.587110	48.992922
1231.341018	178.569740	48.997927
1228.186901	192.442289	49.002932
1224.962100	188.850634	49.007937
1221.276255	178.876297	49.012941
1217.683762	177.739717	49.017946
1214.177296	184.370897	49.022951
1210.224374	183.994668	49.027956
1206.891426	181.390859	49.032961
1203.580795	180.090161	49.037965
1200.115733	184.060972	49.042970
1196.973848	181.596204	49.047975
1192.985534	177.937240	49.052980
1189.723142	175.261318	49.057985
1185.807471	189.377486	49.062989
1182.292634	185.080595	49.067994
1179.136805	172.740540	49.072999
1175.542052	183.388966	49.078004
1172.027615	181.607635	49.083009
1168.980686	179.780208	49.088013
1165.073032	178.810616	49.093018
1161.612225	177.943855	49.098023
1157.665704	178.314903	49.103028
1154.536496	170.808935	49.108033
1151.148109	173.526022	49.113037
1147.532701	184.769211	49.118042
1144.125089	176.412131	49.123047
1140.527823	174.787542	49.128052
1136.931083	176.016580	49.133057
1133.292461	184.717899	49.138061
1129.428085	190.818540	49.143066
1126.622721	187.348492	49.148071
1123.468060	178.912076	49.153076
1119.787474	180.713354	49.158081
1116.322923	183.866659	49.163085
1112.444061	190.662854	49.168090
1109.139561	170.726144	49.173095
1105.593619	182.524952	49.178100
1102.201147	174.326700	49.183105
1098.576638	189.990294	49.188109
1094.659930	184.388879	49.193114
1091.374938	174.496632	49.198119
1088.137367	181.109223	49.203124
1084.338077	179.860845	49.208129
1080.815531	171.599040	49.213133
1077.372576	173.666546	49.218138
1073.979011	178.236880	49.223143
1070.121549	177.570908	49.228148
1066.948290	173.083225	49.233153
1063.484455	178.392551	49.238157
1060.220289	182.061620	49.243162
1056.655458	173.830389	49.248167
1052.822564	177.052131	49.253172
1049.607208	171.897393	49.258177
1046.111570	173.857791	49.263181
1042.386642	179.860964	49.268186
1039.085766	168.548763	49.273191
1035.328620	172.915927	49.278196
1031.805835	174.606256	49.283201
1028.845773	170.657865	49.288205
1025.014416	177.602130	49.293210
1021.458023	168.512412	49.298215
1017.464798	169.297415	49.303220
1013.974969	167.592316	49.308225
1010.959363	166.780875	49.313229
1007.456285	169.661988	49.318234
1004.319076	170.227829	49.323239
1000.446518	175.820029	49.328244
996.899362	176.478616	49.333249
993.340931	174.062597	49.338253
989.922145	180.909463	49.343258
986.351343	173.646379	49.348263
982.821234	171.898914	49.353268
979.029542	179.263831	49.358273
975.778789	172.190210	49.363277
972.119934	180.976133	49.368282
969.031037	166.855280	49.373287
965.370929	177.671046	49.378292
962.038676	167.666917	49.383297
958.598602	163.940077	49.388301
954.526838	169.845569	49.393306
951.700785	172.226223	49.398311
948.228194	172.165362	49.403316
944.672162	174.343747	49.408321
940.760515	175.769805	49.413325
936.835492	171.545420	49.418330
933.606764	172.383895	49.423335
930.213017	172.694189	49.428340
926.594503	164.543925	49.433345
923.266333	170.758469	49.438349
919.846722	163.854335	49.443354
916.781998	166.415980	49.448359
912.811832	176.172599	49.453364
909.150916	164.725578	49.458369
906.010501	173.340191	49.463373
902.243083	173.012043	49.468378
899.266292	162.478676	49.473383
895.263580	173.436771	49.478388
891.381440	167.729156	49.483393
888.317252	168.536340	49.488397
884.788665	177.161686	49.493402
881.516149	163.889554	49.498407
877.954397	179.654238	49.503412
874.500123	170.503255	49.508417
870.631779	167.565489	49.513421
867.062775	169.978585	49.518426
863.859590	162.006221	49.523431
860.048153	176.296203	49.528436
856.825223	173.281960	49.533441
853.393274	162.187845	49.538445
849.620119	171.203221	49.543450
846.433149	163.166135	49.548455
842.618540	165.875612	49.553460
839.336679	172.206555	49.558465
835.710750	168.707289	49.563469
831.904123	168.350041	49.568474
828.829248	173.411548	49.573479
825.104946	167.607768	49.578484
821.723023	170.183655	49.583489
818.433472	168.347624	49.588493
814.665729	168.766398	49.593498
811.254011	158.305298	49.598503
807.631606	174.761232	49.603508
804.169318	162.085092	49.608513
800.478808	161.938356	49.613517
796.976515	165.587669	49.618522
793.766858	165.171818	49.623527
790.338857	161.522003	49.628532
786.889025	156.190866	49.633537
783.509053	166.237992	49.638541
779.892747	171.100066	49.643546
776.259720	160.127108	49.648551
772.779917	163.357578	49.653556
768.984065	160.777960	49.658561
765.542610	154.470642	49.663565
762.083439	162.660453	49.668570
758.526169	158.889348	49.673575
755.135837	168.268921	49.678580
751.868816	161.804452	49.683585
748.447400	167.401596	49.688589
744.506808	169.868720	49.693594
740.661747	159.740958	49.698599
737.382616	161.110721	49.703604
734.456343	155.981817	49.708609
731.008784	157.699139	49.713613
727.471693	166.381100	49.718618
723.796239	170.105513	49.723623
719.952217	170.811495	49.728628
716.479030	163.134388	49.733633
713.225470	161.930865	49.738637
709.101635	170.098567	49.743642
705.814083	165.530506	49.748647
702.145692	157.793307	49.753652
699.190114	166.004060	49.758657
696.136188	167.234444	49.763661
692.367766	170.716934	49.768666
689.066689	167.689049	49.773671
685.256908	166.956037	49.778676
681.715022	155.717313	49.783681
678.290538	164.657918	49.788685
674.143688	168.159014	49.793690
670.995872	166.377786	49.798695
667.532009	168.999046	49.803700
664.276588	166.853403	49.808705
660.481716	166.659263	49.813709
656.755637	166.861012	49.818714
653.715402	160.025000	49.823719
649.874624	180.934339	49.828724
646.787749	161.636333	49.833729
643.222362	166.640020	49.838733
639.693087	168.720714	49.843738
636.189399	160.871116	49.848743
632.134128	163.713388	49.853748
628.769704	160.158428	49.858753
625.537634	156.625315	49.863757
621.817907	170.475633	49.868762
618.531249	162.057760	49.873767
615.072580	166.724488	49.878772
611.927772	162.635748	49.883777
608.403773	162.653897	49.888781
604.291687	158.512910	49.893786
601.126379	159.461428	49.898791
597.812584	162.260573	49.903796
593.528009	163.096315	49.908801
590.564883	154.381546	49.913805
586.682424	156.454601	49.918810
583.673789	155.253507	49.923815
579.942516	161.629879	49.928820
576.809118	145.864663	49.933825
573.546627	163.244123	49.938829
569.774295	154.181091	49.943834
566.070643	154.293752	49.948839
562.213798	157.368474	49.953844
558.724471	162.042561	49.958849
555.506407	153.849284	49.963853
551.969277	160.727128	49.968858
548.557224	167.022379	49.973863
544.983521	158.138662	49.978868
541.547427	160.641747	49.983873
537.721677	157.366561	49.988877
534.152447	164.498524	49.993882
531.099459	162.572860	49.998887
527.343346	173.477380	50.003892
523.910708	157.797030	50.008897
520.730367	162.394744	50.013901
517.201110	161.137809	50.018906
513.707924	157.301903	50.023911
509.425871	177.010839	50.028916
506.075333	164.178813	50.033921
502.903465	165.092353	50.038925
499.665114	175.088287	50.043930
496.006982	158.203039	50.048935
492.252277	159.939054	50.053940
488.699178	157.832118	50.058945
485.490795	159.545672	50.063949
481.910474	157.358788	50.068954
478.851574	154.392235	50.073959
474.753819	161.389751	50.078964
471.487564	157.850923	50.083969
468.188483	157.318399	50.088973
464.429889	166.657111	50.093978
461.094438	154.569842	50.098983
457.468273	168.409409	50.103988
453.932673	164.915475	50.108993
450.274604	160.620177	50.113997
446.514296	163.522256	50.119002
443.242843	157.921136	50.124007
439.628977	151.122977	50.129012
436.108797	159.607329	50.134017
433.081559	162.957065	50.139021
429.522521	158.695440	50.144026
426.204177	156.173196	50.149031
422.327494	171.872172	50.154036
418.557438	163.048395	50.159041
415.132346	161.477656	50.164045
411.622930	168.992049	50.169050
408.221485	155.363087	50.174055
404.843904	165.790087	50.179060
401.310627	162.325397	50.184065
397.671633	154.372321	50.189069
393.620424	167.153618	50.194074
390.644014	150.230325	50.199079
387.445699	160.589931	50.204084
384.277874	157.375741	50.209089
380.601823	153.543584	50.214093
377.004504	160.675229	50.219098
373.309453	148.201705	50.224103
369.507116	157.213047	50.229108
365.913751	163.351087	50.234113
363.083509	159.176871	50.239117
359.240443	160.368187	50.244122
356.266069	148.150211	50.249127
352.581245	147.454467	50.254132
348.496213	153.147216	50.259137
345.318779	158.683324	50.264141
341.725924	159.040822	50.269146
338.305511	157.009819	50.274151
334.512498	162.830632	50.279156
331.352888	151.362758	50.284161
327.778301	148.032499	50.289165
324.034710	153.984451	50.294170
320.745913	155.259036	50.299175
317.075586	160.660236	50.304180
313.870342	161.144018	50.309185
310.679235	154.556966	50.314189
306.608681	151.346244	50.319194
303.267648	152.168159	50.324199
300.060037	154.223511	50.329204
296.198935	147.379475	50.334209
292.577289	148.053406	50.339213
289.048131	154.158281	50.344218
285.734994	146.867283	50.349223
281.945736	145.222909	50.354228
278.665598	142.600616	50.359233
275.326778	147.777575	50.364237
271.653511	152.528853	50.369242
268.178781	150.331654	50.374247
264.541331	158.704445	50.379252
260.919208	153.261106	50.384257
257.937962	141.213522	50.389261
254.243680	146.496375	50.394266
251.097422	151.463758	50.399271
247.236207	150.137220	50.404276
243.584621	149.049225	50.409281
239.841223	152.027743	50.414285
236.390106	154.260290	50.419290
233.052663	154.905944	50.424295
229.330567	150.616234	50.429300
226.283818	152.658658	50.434305
223.054082	154.058197	50.439309
219.461473	140.286738	50.444314
215.578145	144.719073	50.449319
211.774082	154.074982	50.454324
208.344959	145.770086	50.459329
205.083667	146.979117	50.464333
201.837033	135.518611	50.469338
198.502575	141.944932	50.474343
194.627685	156.083477	50.479348
191.251723	142.995529	50.484353
187.756813	147.419345	50.489357
183.652616	156.684080	50.494362
180.494574	143.037954	50.499367
177.010863	148.753777	50.504372
173.775332	152.813625	50.509377
170.292234	136.516908	50.514381
166.665628	154.800341	50.519386
163.044910	151.954303	50.524391
159.441792	146.567279	50.529396
156.077977	148.939244	50.534401
152.621798	143.941111	50.539405
149.157597	152.164970	50.544410
145.980489	140.042481	50.549415
142.352991	139.007193	50.554420
138.451173	143.525990	50.559425
135.044135	143.033182	50.564429
131.314094	145.519537	50.569434
128.244650	146.973632	50.574439
124.716363	149.500250	50.579444
120.661749	136.168055	50.584449
117.597672	132.980476	50.589453
113.917066	146.913118	50.594458
110.597178	143.450044	50.599463
106.830122	140.099830	50.604468
103.600480	141.720694	50.609473
100.031934	146.330550	50.614477
96.364830	148.057739	50.619482
93.497850	143.383635	50.624487
89.567181	141.141718	50.629492
85.910055	143.929573	50.634497
82.746388	145.703804	50.639501
78.546651	141.457505	50.644506
75.304921	136.125655	50.649511
71.975503	142.639103	50.654516
68.445219	139.709714	50.659521
65.213993	131.709810	50.664525
61.250179	144.999088	50.669530
57.872665	148.492400	50.674535
54.820950	146.035808	50.679540
50.926280	148.505019	50.684545
47.610584	139.583837	50.689549
43.875940	145.534059	50.694554
40.532008	140.094910	50.699559
37.322391	151.501360	50.704564
33.467455	136.116983	50.709569
30.436347	137.327920	50.714573
26.897196	150.894601	50.719578
22.696577	144.149478	50.724583
19.495873	150.236312	50.729588
15.452023	152.053330	50.734593
12.446481	143.798919	50.739597
8.794729	140.626331	50.744602
5.515343	144.781897	50.749607
2.062121	141.837248	50.754612