Thu Jun 16 11:13:38 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.136408	111.256736	0.000000
0.492191	111.046140	0.005005
0.383751	103.043530	0.010010
-0.023689	105.353984	0.015014
0.099316	95.542589	0.020019
-0.783567	69.173268	0.025024
-0.667853	72.804457	0.030029
-0.990949	67.877549	0.035034
-1.165818	59.320260	0.040038
-1.399174	53.843430	0.045043
-1.662160	52.650988	0.050048
-2.109360	25.040403	0.055053
-2.551095	26.561072	0.060058
-2.424037	17.160935	0.065062
-2.799841	14.076720	0.070067
-3.296137	20.888795	0.075072
-3.768946	15.936432	0.080077
-3.870145	20.309813	0.085082
-3.728345	20.547148	0.090086
-4.397120	12.262601	0.095091
-4.956041	17.241195	0.100096
-5.111504	20.375974	0.105101
-5.703151	15.787649	0.110106
-5.330721	10.960585	0.115110
-5.550557	11.227596	0.120115
-5.679709	7.912910	0.125120
-5.544388	14.447662	0.130125
-6.353867	22.713062	0.135130
-6.904177	8.898364	0.140134
-6.914421	0.327517	0.145139
-7.050001	15.705819	0.150144
-7.087053	9.862030	0.155149
-8.287073	13.054502	0.160154
-8.196440	15.030967	0.165158
-8.521154	9.379146	0.170163
-8.815499	10.951617	0.175168
-8.372470	11.538617	0.180173
-8.834563	11.795054	0.185178
-8.985717	10.805414	0.190182
-9.455979	17.686683	0.195187
-10.141871	5.795640	0.200192
-9.971987	5.361241	0.205197
-10.070996	18.570728	0.210202
-10.051542	16.481222	0.215206
-10.513769	6.076620	0.220211
-11.292179	5.195575	0.225216
-11.543974	-2.218005	0.230221
-11.998159	7.652555	0.235226
-12.029198	6.289393	0.240230
-11.955438	4.731534	0.245235
-11.935080	3.829270	0.250240
-11.725386	-2.730375	0.255245
-12.053044	12.396532	0.260250
-12.452005	3.824319	0.265254
-12.817823	5.308271	0.270259
-13.558093	9.962076	0.275264
-14.210699	-1.178284	0.280269
-14.513006	15.831967	0.285274
-14.714187	13.591089	0.290278
-14.528380	1.811799	0.295283
-14.738256	2.193969	0.300288
-14.842926	10.396848	0.305293
-14.688737	8.155742	0.310298
-15.213385	6.818713	0.315302
-15.794764	12.145810	0.320307
-15.902161	4.018087	0.325312
-16.154686	13.068959	0.330317
-16.227858	7.439990	0.335322
-16.334419	4.440815	0.340326
-17.316381	9.543480	0.345331
-17.750428	5.551814	0.350336
-17.448935	6.170097	0.355341
-18.134407	12.237031	0.360346
-17.923947	1.787756	0.365350
-17.904642	5.677054	0.370355
-18.003125	19.855130	0.375360
-18.273867	8.233761	0.380365
-19.157138	12.175642	0.385370
-19.291760	17.164715	0.390374
-19.455291	14.478903	0.395379
-19.722312	18.004534	0.400384
-19.470774	15.014839	0.405389
-20.608368	12.318545	0.410394
-20.793865	6.788148	0.415398
-20.860831	10.622450	0.420403
-21.127117	15.277243	0.425408
-20.782359	7.882665	0.430413
-21.445685	15.585262	0.435418
-22.194514	9.605468	0.440422
-22.396794	7.125242	0.445427
-22.551235	14.651004	0.450432
-22.708456	5.287203	0.455437
-22.550343	8.280283	0.460442
-22.777624	12.348943	0.465446
-22.727896	14.584128	0.470451
-22.811038	12.237125	0.475456
-23.551597	12.919201	0.480461
-23.894268	2.866867	0.485466
-23.919637	9.861160	0.490470
-24.721802	7.017292	0.495475
-25.214271	10.364721	0.500480
-25.698978	11.545528	0.505485
-25.349720	14.585154	0.510490
-25.724046	23.725613	0.515494
-25.666253	11.822058	0.520499
-25.779117	-0.161506	0.525504
-25.703579	6.447837	0.530509
-26.110923	13.184438	0.535514
-27.115272	19.362083	0.540518
-27.595476	7.973428	0.545523
-28.031276	22.662437	0.550528
-27.727964	2.593823	0.555533
-27.948292	7.007802	0.560538
-28.068959	7.168551	0.565542
-27.859880	13.819458	0.570547
-27.981897	8.992227	0.575552
-28.219163	8.699105	0.580557
-29.105764	20.001958	0.585562
-29.139137	0.438848	0.590566
-29.528124	11.984914	0.595571
-29.722417	22.355124	0.600576
-29.640435	3.851226	0.605581
-30.703362	18.568404	0.610586
-30.835441	7.889246	0.615590
-30.857783	9.019291	0.620595
-31.191255	16.703186	0.625600
-30.957700	1.290205	0.630605
-31.114286	10.799741	0.635610
-31.349278	20.173176	0.640614
-31.731895	17.599041	0.645619
-32.375676	14.934887	0.650624
-32.488868	16.244006	0.655629
-32.366067	17.096822	0.660634
-33.228259	19.584329	0.665638
-33.671677	24.098812	0.670643
-34.103598	22.704728	0.675648
-34.014474	5.206603	0.680653
-34.132539	22.213046	0.685658
-34.100495	17.029075	0.690662
-34.037850	21.107731	0.695667
-34.506327	30.026097	0.700672
-34.866585	7.332374	0.705677
-35.584392	24.454017	0.710682
-35.708382	10.155511	0.715686
-35.658545	14.138122	0.720691
-35.767970	8.464043	0.725696
-35.938939	7.482908	0.730701
-36.604350	18.753348	0.735706
-37.120246	10.971140	0.740710
-36.901422	18.186707	0.745715
-37.069017	21.684957	0.750720
-37.346761	14.005746	0.755725
-37.771434	22.423800	0.760730
-38.393894	16.262218	0.765734
-38.592747	16.931325	0.770739
-38.892007	22.354356	0.775744
-38.837193	15.277707	0.780749
-38.740166	24.484992	0.785754
-38.956013	15.099207	0.790758
-38.699761	6.840554	0.795763
-39.777494	24.894563	0.800768
-39.801112	20.606979	0.805773
-40.596139	9.301628	0.810778
-40.302843	17.162806	0.815782
-40.695110	16.452248	0.820787
-41.573163	15.543379	0.825792
-41.480000	16.215821	0.830797
-41.999623	18.900055	0.835802
-42.133004	11.806072	0.840806
-41.809670	20.187023	0.845811
-42.232019	13.271512	0.850816
-42.000682	22.296286	0.855821
-42.575772	30.700531	0.860826
-43.154799	23.974970	0.865830
-43.543088	16.288575	0.870835
-43.713056	25.949889	0.875840
-43.440369	15.477498	0.880845
-43.601834	20.566504	0.885850
-44.368445	19.620374	0.890854
-44.784767	19.887204	0.895859
-45.182533	24.968108	0.900864
-45.231557	18.895152	0.905869
-45.204124	18.138416	0.910874
-45.390430	16.751884	0.915878
-45.171773	19.088288	0.920883
-46.078720	19.475269	0.925888
-46.622159	12.551162	0.930893
-46.955064	15.907343	0.935898
-46.919289	14.977670	0.940902
-46.843544	24.455427	0.945907
-46.994117	19.759189	0.950912
-46.972570	20.886322	0.955917
-48.044208	21.793492	0.960922
-48.569606	17.912814	0.965926
-48.553565	20.989653	0.970931
-48.675298	17.033482	0.975936
-48.300464	8.741122	0.980941
-48.547846	23.816788	0.985946
-49.165341	32.250732	0.990950
-49.775597	19.490286	0.995955
-50.266048	22.447014	1.000960
-49.913409	15.810761	1.005965
-49.906869	15.061326	1.010970
-50.511960	13.338739	1.015974
-50.985867	10.413494	1.020979
-51.823303	30.517172	1.025984
-51.646471	20.130664	1.030989
-51.616042	20.267922	1.035994
-51.921770	22.738146	1.040998
-51.733664	15.729145	1.046003
-52.303711	24.213844	1.051008
-52.054114	21.854369	1.056013
-52.876288	16.924136	1.061018
-53.226362	14.984293	1.066022
-53.507199	23.221421	1.071027
-53.545683	21.321533	1.076032
-53.403448	21.156191	1.081037
-54.072196	21.603940	1.086042
-54.718055	27.651215	1.091046
-55.093606	16.050029	1.096051
-55.049590	20.211671	1.101056
-54.394933	11.478649	1.106061
-54.860558	21.593103	1.111066
-55.383051	9.827977	1.116070
-55.894735	11.416341	1.121075
-56.876847	14.534530	1.126080
-56.660439	10.665820	1.131085
-56.833014	19.182690	1.136090
-56.952471	18.500543	1.141094
-56.720349	5.527296	1.146099
-57.267262	15.426601	1.151104
-56.854786	11.447453	1.156109
-57.495993	0.232905	1.161114
-58.155075	17.065052	1.166118
-58.124242	12.751700	1.171123
-58.404748	12.827487	1.176128
-58.982102	11.640048	1.181133
-59.643194	20.657524	1.186138
-59.652445	8.990675	1.191142
-59.589178	9.555199	1.196147
-60.288592	9.833104	1.201152
-59.988760	15.090924	1.206157
-60.360638	17.760508	1.211162
-60.468941	20.001685	1.216166
-59.986355	9.194604	1.221171
-61.026161	16.655571	1.226176
-61.245324	13.296079	1.231181
-61.440342	8.835574	1.236186
-61.685880	8.039998	1.241190
-61.798848	6.801264	1.246195
-62.846040	13.004439	1.251200
-63.259900	7.372685	1.256205
-63.092618	17.511772	1.261210
-63.222749	7.757467	1.266214
-63.118888	15.857810	1.271219
-63.440488	15.237879	1.276224
-63.215484	8.242811	1.281229
-63.441906	15.566587	1.286234
-64.259756	12.799898	1.291238
-64.403161	6.217910	1.296243
-64.419835	22.099420	1.301248
-65.241638	7.429691	1.306253
-65.607379	14.883729	1.311258
-66.028031	12.201447	1.316262
-66.106388	9.029802	1.321267
-66.352559	19.752092	1.326272
-66.355265	20.224427	1.331277
-65.989768	7.801521	1.336282
-66.772177	22.314102	1.341286
-67.596457	12.373624	1.346291
-67.830733	21.059326	1.351296
-67.871500	11.436158	1.356301
-68.141932	21.204536	1.361306
-68.069883	14.850932	1.366310
-68.217305	16.277582	1.371315
-68.222109	22.166621	1.376320
-68.130074	12.700559	1.381325
-68.919945	18.718656	1.386330
-69.412549	16.070955	1.391334
-69.446764	9.947118	1.396339
-69.992344	14.692562	1.401344
-69.946973	20.951249	1.406349
-70.718697	21.220191	1.411354
-71.252712	18.678086	1.416358
-71.101703	7.434218	1.421363
-71.352415	16.416226	1.426368
-71.141766	13.895675	1.431373
-71.282653	15.333084	1.436378
-71.226058	24.721465	1.441382
-71.842959	12.881872	1.446387
-72.698025	20.859441	1.451392
-72.660925	14.716516	1.456397
-72.940484	11.156974	1.461402
-73.007525	15.775778	1.466406
-72.666732	19.346272	1.471411
-73.884227	16.797263	1.476416
-74.300496	9.743330	1.481421
-74.421088	8.242550	1.486426
-74.760554	11.392545	1.491430
-74.471837	5.965596	1.496435
-74.867158	9.363562	1.501440
-74.482360	7.941639	1.506445
-75.233589	5.637084	1.511450
-76.249438	-2.283663	1.516454
-76.093777	16.174588	1.521459
-76.306277	23.844707	1.526464
-75.951222	3.238668	1.531469
-76.290387	10.093334	1.536474
-76.463250	18.435831	1.541478
-77.010903	10.694788	1.546483
-77.720974	11.887886	1.551488
-77.259547	12.291305	1.556493
-77.630651	9.691301	1.561498
-77.967410	14.822692	1.566502
-78.549102	10.721659	1.571507
-78.648187	9.241002	1.576512
-78.951054	11.925126	1.581517
-79.021144	19.568944	1.586522
-79.455228	10.441206	1.591526
-79.508966	8.970911	1.596531
-79.822808	8.470352	1.601536
-80.686684	13.235944	1.606541
-81.005817	16.919845	1.611546
-81.028292	10.270615	1.616550
-80.899753	0.140611	1.621555
-81.081397	19.237652	1.626560
-80.842236	5.458924	1.631565
-81.052127	12.061376	1.636570
-82.095584	18.537207	1.641574
-82.346541	7.460499	1.646579
-82.536176	14.057237	1.651584
-82.467393	5.612533	1.656589
-82.500015	9.224811	1.661594
-83.101318	11.209185	1.666598
-83.798985	9.307457	1.671603
-84.272871	14.162592	1.676608
-84.160186	5.356566	1.681613
-84.321077	8.355309	1.686618
-84.626978	17.889227	1.691622
-84.612371	13.544326	1.696627
-84.620467	12.916482	1.701632
-84.188182	16.537063	1.706637
-84.845747	4.378052	1.711642
-85.743474	11.572259	1.716646
-85.547579	8.047293	1.721651
-86.091421	16.309732	1.726656
-86.686181	7.442755	1.731661
-87.242220	15.335188	1.736666
-87.936663	10.811022	1.741670
-86.565801	1.454728	1.746675
-87.294391	19.262007	1.751680
-87.442011	10.467628	1.756685
-87.564533	12.224301	1.761690
-87.992294	21.036094	1.766694
-88.530467	7.937112	1.771699
-89.142936	7.377292	1.776704
-89.117852	6.653303	1.781709
-88.981764	2.973275	1.786714
-89.078139	6.983993	1.791718
-89.094091	6.751962	1.796723
-89.819518	4.762484	1.801728
-89.707890	10.656050	1.806733
-89.973310	0.417035	1.811738
-91.214509	13.839157	1.816742
-90.782685	3.750774	1.821747
-91.787482	9.588142	1.826752
-92.072124	9.622982	1.831757
-91.519328	12.470031	1.836762
-92.083324	3.039893	1.841766
-92.144308	7.121908	1.846771
-92.056709	4.998058	1.851776
-92.286370	8.976940	1.856781
-92.655532	0.289029	1.861786
-93.326134	5.377434	1.866790
-93.376208	14.981138	1.871795
-93.581367	9.324168	1.876800
-94.072185	5.358664	1.881805
-93.757077	8.791732	1.886810
-94.784196	10.127697	1.891814
-94.602919	6.683281	1.896819
-95.102743	11.574470	1.901824
-95.438634	2.340638	1.906829
-95.261845	-2.295356	1.911834
-95.228958	16.476281	1.916838
-95.246843	7.670427	1.921843
-96.647184	11.401519	1.926848
-96.824086	17.585164	1.931853
-96.975712	11.038275	1.936858
-97.270457	7.857213	1.941862
-97.108086	14.199749	1.946867
-97.150936	3.591190	1.951872
-97.305741	10.811281	1.956877
-97.893758	6.487354	1.961882
-98.236917	5.077818	1.966886
-98.554920	0.069896	1.971891
-98.911365	5.369979	1.976896
-98.867167	8.918753	1.981901
-98.847472	13.800830	1.986906
-99.447652	10.337491	1.991910
-100.022116	6.581836	1.996915
-100.243028	10.237098	2.006912
-99.283792	4.239072	2.016909
-99.056856	5.435427	2.026906
-99.042800	11.109323	2.036902
-98.182883	6.809679	2.046899
-97.750545	11.983075	2.056896
-97.294861	13.784875	2.066893
-96.514360	5.989562	2.076890
-96.297088	10.953628	2.086886
-95.197245	13.704275	2.096883
-94.846481	13.528812	2.106880
-94.868185	7.785368	2.116877
-94.378703	13.748791	2.126874
-93.387333	4.233796	2.136870
-93.246826	2.633666	2.146867
-92.851919	8.859667	2.156864
-91.974275	8.789892	2.166861
-91.635224	9.410107	2.176858
-91.322907	4.457604	2.186854
-90.267222	12.403397	2.196851
-90.347089	7.103899	2.206848
-89.699411	5.079800	2.216845
-88.934760	8.710506	2.226842
-88.419933	6.379083	2.236838
-88.423609	12.680889	2.246835
-87.587278	15.398289	2.256832
-87.237368	7.259119	2.266829
-86.448666	6.307769	2.276826
-85.715986	1.920449	2.286822
-85.512159	7.435556	2.296819
-85.431330	7.944452	2.306816
-84.858438	9.816622	2.316813
-84.263867	0.284383	2.326810
-83.447462	11.143069	2.336806
-82.642540	5.803873	2.346803
-82.602932	6.686349	2.356800
-82.490043	9.504793	2.366797
-81.499091	3.926477	2.376794
-80.734783	2.533763	2.386790
-80.916523	1.489186	2.396787
-80.107633	5.196445	2.406784
-79.292947	5.569434	2.416781
-79.220124	9.892392	2.426778
-78.719866	9.836984	2.436774
-77.962128	9.457648	2.446771
-77.882935	13.409773	2.456768
-76.915136	7.109944	2.466765
-76.313598	8.505660	2.476762
-76.162278	8.785788	2.486758
-75.868395	12.603207	2.496755
-75.015910	11.741874	2.506752
-74.693131	7.624994	2.516749
-73.806754	6.304811	2.526746
-73.041487	15.032045	2.536742
-73.286547	10.703784	2.546739
-73.062546	10.318276	2.556736
-72.340746	9.381393	2.566733
-71.597918	3.151147	2.576730
-70.450859	5.334952	2.586726
-70.741256	13.365027	2.596723
-70.142125	11.080815	2.606720
-69.782966	7.543587	2.616717
-68.917832	8.044902	2.626714
-68.568745	0.889269	2.636710
-68.183545	13.269210	2.646707
-66.991817	17.578383	2.656704
-66.967187	10.435574	2.666701
-66.700621	12.781200	2.676698
-66.386638	6.011421	2.686694
-65.464470	13.259284	2.696691
-65.292915	5.939283	2.706688
-64.314108	11.872612	2.716685
-63.941816	12.459677	2.726682
-63.652912	12.651033	2.736678
-63.030121	10.721678	2.746675
-62.336382	12.678685	2.756672
-62.212312	14.577967	2.766669
-61.535744	14.391135	2.776666
-61.172239	17.418963	2.786662
-60.743060	16.319350	2.796659
-59.475580	19.233488	2.806656
-59.242969	15.112345	2.816653
-59.211779	10.514642	2.826650
-58.779440	11.355574	2.836646
-57.752646	14.092471	2.846643
-57.329155	11.382359	2.856640
-57.376491	5.098134	2.866637
-56.367399	3.623282	2.876634
-55.936039	5.959106	2.886630
-55.695687	12.200878	2.896627
-55.025159	16.723667	2.906624
-54.692771	8.025237	2.916621
-54.252282	1.977226	2.926618
-53.176193	11.685635	2.936614
-52.870032	8.482595	2.946611
-52.487086	11.850568	2.956608
-52.432570	12.240387	2.966605
-51.586397	8.796523	2.976602
-51.121463	8.612763	2.986598
-50.100751	7.671524	2.996595
-49.740240	13.352275	3.006592
-49.603942	8.582216	3.016589
-49.394407	10.476165	3.026586
-48.191757	15.559993	3.036582
-47.930101	13.066630	3.046579
-47.810633	14.592743	3.056576
-46.803639	23.263295	3.066573
-46.429950	9.149017	3.076570
-46.111597	14.058847	3.086566
-45.371633	12.661023	3.096563
-44.532246	12.669192	3.106560
-44.670640	15.509412	3.116557
-44.612452	22.503669	3.126554
-43.569970	13.123948	3.136550
-42.708328	19.438280	3.146547
-42.268949	21.198923	3.156544
-42.013821	23.328633	3.166541
-41.404766	16.402562	3.176538
-41.178450	7.770508	3.186534
-40.309309	16.665301	3.196531
-40.213241	8.200275	3.206528
-39.583972	15.470622	3.216525
-38.434683	14.122303	3.226522
-38.446526	6.388695	3.236518
-38.160876	12.056086	3.246515
-37.707869	9.513418	3.256512
-36.909196	17.489504	3.266509
-36.568015	8.805819	3.276506
-35.613540	19.846574	3.286502
-35.097745	18.050969	3.296499
-34.936525	8.027843	3.306496
-34.892906	16.455525	3.316493
-33.969092	5.942218	3.326490
-33.761710	10.008340	3.336486
-33.239468	8.376682	3.346483
-32.129221	8.306702	3.356480
-32.120680	10.342329	3.366477
-30.942163	10.881500	3.376474
-30.714677	11.062067	3.386470
-30.531385	10.338153	3.396467
-30.402598	11.848305	3.406464
-29.333049	14.568164	3.416461
-28.907705	6.276260	3.426458
-28.672886	5.273717	3.436454
-27.780087	6.270438	3.446451
-27.384588	7.028510	3.456448
-27.050229	15.432393	3.466445
-26.427258	15.833617	3.476442
-25.764764	11.095130	3.486438
-25.463750	14.805533	3.496435
-25.088558	10.965908	3.506432
-24.240603	8.708489	3.516429
-23.753976	12.904093	3.526426
-23.848126	11.587025	3.536422
-22.900891	12.737984	3.546419
-22.412917	7.855229	3.556416
-22.005447	10.183992	3.566413
-21.101847	9.594258	3.576410
-20.821892	10.329642	3.586406
-20.822247	9.356779	3.596403
-19.500993	12.240405	3.606400
-19.129770	13.635024	3.616397
-18.996766	15.490900	3.626394
-19.000129	10.112817	3.636390
-17.727452	7.224634	3.646387
-17.203531	13.047247	3.656384
-17.338501	2.503953	3.666381
-16.348890	-2.551540	3.676378
-16.141126	6.408992	3.686374
-15.429698	0.741698	3.696371
-14.773697	1.263901	3.706368
-14.600899	5.901794	3.716365
-13.916219	4.274360	3.726362
-13.375995	0.621865	3.736358
-13.034179	3.531880	3.746355
-11.976421	6.994240	3.756352
-11.608758	3.242096	3.766349
-11.552684	-2.071375	3.776346
-11.283447	-2.360934	3.786342
-10.165345	7.494143	3.796339
-9.696812	8.271558	3.806336
-9.359800	5.505607	3.816333
-9.360339	1.610581	3.826330
-8.253632	4.417352	3.836326
-8.099538	-9.498870	3.846323
-7.334776	-1.957148	3.856320
-6.725429	0.303728	3.866317
-6.419089	-0.162950	3.876314
-6.100288	5.143160	3.886310
-5.321495	1.844975	3.896307
-5.056453	3.123493	3.906304
-4.173465	16.770956	3.916301
-3.730295	18.861788	3.926298
-3.455046	25.008951	3.936294
-3.526428	22.955964	3.946291
-2.889569	45.666714	3.956288
-2.127214	47.606417	3.966285
-1.845492	58.516970	3.976282
-1.271929	71.485290	3.986278
-0.725755	93.775627	3.996275
-0.488004	107.279150	4.006272
0.000000	120.521011	4.011277
-0.115121	120.723166	4.016282
0.092565	135.292920	4.021286
0.564666	146.384446	4.026291
0.660463	156.851535	4.031296
0.624232	158.712743	4.036301
0.395955	158.328552	4.041306
0.596006	155.050390	4.046310
0.582360	165.861722	4.051315
0.646240	164.732060	4.056320
0.763348	169.610130	4.061325
1.043938	171.729743	4.066330
1.371006	171.858329	4.071334
1.313254	176.750797	4.076339
0.875619	173.488042	4.081344
1.060566	160.477270	4.086349
0.874070	155.624934	4.091354
0.721366	150.416497	4.096358
0.715047	172.029452	4.101363
1.222479	171.321042	4.106368
1.008585	179.679784	4.111373
1.216919	187.834583	4.116378
1.765743	176.695021	4.121382
1.044317	173.330197	4.126387
0.708256	156.385566	4.131392
1.094775	161.567458	4.136397
0.803453	166.692082	4.141402
1.210002	169.185495	4.146406
0.929969	165.038405	4.151411
0.929843	176.148306	4.156416
1.334361	186.037385	4.161421
0.843779	196.644912	4.166426
1.351318	187.140950	4.171430
1.217647	191.945045	4.176435
1.578984	189.397196	4.181440
1.632660	179.745680	4.186445
1.267178	179.716924	4.191450
1.027611	161.743062	4.196454
1.130850	169.087806	4.201459
1.092658	179.358239	4.206464
1.342679	180.949974	4.211469
1.387521	191.557211	4.216474
1.611928	183.193823	4.221478
1.137320	166.880083	4.226483
1.006444	181.039690	4.231488
1.278726	180.878803	4.236493
1.282845	186.036886	4.241498
1.691748	194.558882	4.246502
1.894888	198.753472	4.251507
1.256477	174.491274	4.256512
1.250383	172.420175	4.261517
1.036177	164.306269	4.266522
1.376052	173.810024	4.271526
1.340766	191.187731	4.276531
1.617851	190.624723	4.281536
1.801629	190.579090	4.286541
1.549423	199.429060	4.291546
1.490241	174.509401	4.296550
1.000994	184.374523	4.301555
1.649612	192.625459	4.306560
1.675916	188.954058	4.311565
1.732519	192.774990	4.316570
1.814086	185.631292	4.321574
1.021042	189.732429	4.326579
1.524745	195.473477	4.331584
1.340028	195.759547	4.336589
1.137379	203.230625	4.341594
1.779468	201.390689	4.346598
1.343483	195.785797	4.351603
1.707934	203.228367	4.356608
1.564190	205.066407	4.361613
1.228156	200.071056	4.366618
1.610731	193.483448	4.371622
1.517996	201.816062	4.376627
1.510362	201.279686	4.381632
1.212320	199.315924	4.386637
1.500887	219.088352	4.391642
1.733779	220.893254	4.396646
1.720712	227.149060	4.401651
1.574189	238.953954	4.406656
2.114215	234.751034	4.411661
2.145322	237.391249	4.416666
2.198491	237.142661	4.421670
1.861415	210.061470	4.426675
1.579400	203.798754	4.431680
1.900670	213.993922	4.436685
1.770703	220.219124	4.441690
2.277006	223.943450	4.446694
1.955565	206.588510	4.451699
1.489311	202.877456	4.456704
1.758149	213.212301	4.461709
1.771398	228.840086	4.466714
1.601070	232.745885	4.471718
2.203263	231.559418	4.476723
1.976181	230.321665	4.481728
2.181055	226.452539	4.486733
2.248390	229.041680	4.491738
2.282853	216.684555	4.496742
1.589988	217.048386	4.501747
2.351361	227.138472	4.506752
2.263184	213.694219	4.511757
1.919341	210.615928	4.516762
1.814457	190.188336	4.521766
1.995317	215.349601	4.526771
2.095012	221.991056	4.531776
2.047552	217.682395	4.536781
2.282042	221.382977	4.541786
2.424399	219.185231	4.546790
2.205267	209.417282	4.551795
1.889424	210.761191	4.556800
2.450200	204.378926	4.561805
1.803384	207.078981	4.566810
2.052309	213.050372	4.571814
1.999562	223.468360	4.576819
2.212077	233.603773	4.581824
2.419523	230.794956	4.586829
2.063233	241.777702	4.591834
2.021221	228.895438	4.596838
2.073940	237.163388	4.601843
1.855192	236.886930	4.606848
2.300175	225.438933	4.611853
2.175093	237.693601	4.616858
2.389064	235.390296	4.621862
2.491911	233.579391	4.626867
2.240444	228.355679	4.631872
2.292956	225.425570	4.636877
2.348115	241.987411	4.641882
2.605760	225.953431	4.646886
2.622012	238.311316	4.651891
2.339857	235.936296	4.656896
2.169753	217.598199	4.661901
1.872467	242.946555	4.666906
2.197612	236.718544	4.671910
2.049823	242.127867	4.676915
2.051577	238.078619	4.681920
2.380763	238.199852	4.686925
2.368219	255.336115	4.691930
2.628061	253.081263	4.696934
2.810101	253.912070	4.701939
2.701106	250.584628	4.706944
2.699653	247.398939	4.711949
2.266625	244.824017	4.716954
2.608474	251.181296	4.721958
2.702002	259.172693	4.726963
2.257778	255.816005	4.731968
2.688211	253.622539	4.736973
2.681249	267.257720	4.741978
2.656895	260.557583	4.746982
2.608592	257.047464	4.751987
2.591239	265.800355	4.756992
3.268661	259.837509	4.761997
2.452394	251.948344	4.767002
2.317917	244.702206	4.772006
2.501769	259.893990	4.777011
2.605999	253.748652	4.782016
2.873361	255.291063	4.787021
2.613654	264.791065	4.792026
2.505568	249.533834	4.797030
2.673916	257.360049	4.802035
2.780266	275.502599	4.807040
2.552198	263.285405	4.812045
2.618036	258.711470	4.817050
2.425882	264.507263	4.822054
2.725439	258.039302	4.827059
2.476942	267.022376	4.832064
2.780713	265.680712	4.837069
2.805594	273.117281	4.842074
2.762310	264.241674	4.847078
2.657988	272.380411	4.852083
2.882152	283.734491	4.857088
3.451669	274.185013	4.862093
3.103605	270.144437	4.867098
2.902859	257.939800	4.872102
3.112161	261.753173	4.877107
2.925514	270.076780	4.882112
2.913161	264.858230	4.887117
2.830768	266.472451	4.892122
3.049898	259.392112	4.897126
3.029434	257.190883	4.902131
2.710814	263.538338	4.907136
2.828530	271.015698	4.912141
2.709533	281.404620	4.917146
2.845896	295.482581	4.922150
3.180302	290.574898	4.927155
3.135616	295.015080	4.932160
3.168259	298.045331	4.937165
3.083462	290.511274	4.942170
3.464597	292.826989	4.947174
3.428641	297.150401	4.952179
3.066204	291.702512	4.957184
3.419666	287.341387	4.962189
3.115648	276.360846	4.967194
3.061883	273.770794	4.972198
2.974815	285.986168	4.977203
2.872403	284.996150	4.982208
3.226832	284.605336	4.987213
3.463964	287.982106	4.992218
3.421814	295.615037	4.997222
3.326582	291.260681	5.002227
3.290403	294.801104	5.007232
3.756958	290.325100	5.012237
3.082422	277.618555	5.017242
3.304737	281.861891	5.022246
3.591042	281.563528	5.027251
3.220672	280.621345	5.032256
3.304865	273.817433	5.037261
2.871754	287.995516	5.042266
3.074718	294.216733	5.047270
3.589099	304.573115	5.052275
3.199521	305.073581	5.057280
3.537479	301.500211	5.062285
3.600383	309.364694	5.067290
3.495277	308.778422	5.072294
3.530763	298.389331	5.077299
3.071766	305.581306	5.082304
3.132880	301.767685	5.087309
3.371633	305.087267	5.092314
3.595046	295.195223	5.097318
3.699224	298.563483	5.102323
3.082098	298.479829	5.107328
3.295175	293.057189	5.112333
3.026036	303.575611	5.117338
3.424908	291.167971	5.122342
3.361034	302.456903	5.127347
3.309475	318.748587	5.132352
3.903140	322.019386	5.137357
3.834610	321.334530	5.142362
3.754323	307.286107	5.147366
3.512278	313.366693	5.152371
3.354163	306.280110	5.157376
3.535386	306.430729	5.162381
3.111316	325.296531	5.167386
3.438634	324.092640	5.172390
3.622677	327.965747	5.177395
3.696527	318.126817	5.182400
4.029274	319.892341	5.187405
3.962113	328.965053	5.192410
3.791838	320.155782	5.197414
3.927823	326.335004	5.202419
3.758739	327.712975	5.207424
3.926489	322.056406	5.212429
3.765255	336.642135	5.217434
4.043477	321.733173	5.222438
4.236102	320.118643	5.227443
4.105924	316.747629	5.232448
3.468126	306.094318	5.237453
3.828070	309.820260	5.242458
4.081960	320.584825	5.247462
3.845708	318.687294	5.252467
3.932059	314.370304	5.257472
3.832107	312.849507	5.262477
3.470104	325.608853	5.267482
3.623850	320.545939	5.272486
4.320102	322.353696	5.277491
3.907907	326.421329	5.282496
3.960633	322.047839	5.287501
3.736158	321.971905	5.292506
3.801496	323.111160	5.297510
3.866646	318.939539	5.302515
3.969032	321.665460	5.307520
3.764990	317.970929	5.312525
4.178319	322.674013	5.317530
3.880603	325.165946	5.322534
4.063282	324.870699	5.327539
3.759463	323.180460	5.332544
3.957544	324.490650	5.337549
3.741621	327.285552	5.342554
4.078140	335.646351	5.347558
4.217761	347.828949	5.352563
3.958228	347.308742	5.357568
3.996639	338.403215	5.362573
3.671461	355.804746	5.367578
3.840263	351.751736	5.372582
3.992259	362.132529	5.377587
3.735028	359.404230	5.382592
4.131211	348.034943	5.387597
4.010001	363.853491	5.392602
4.179034	361.211116	5.397606
4.295214	356.306920	5.402611
3.976083	359.748109	5.407616
4.290036	368.405464	5.412621
4.404005	385.078396	5.417626
4.160384	372.919722	5.422630
4.621171	379.265883	5.427635
4.477696	382.292502	5.432640
4.344530	358.347157	5.437645
4.053325	369.041226	5.442650
4.494872	382.792992	5.447654
4.255534	385.410840	5.452659
4.316805	385.838084	5.457664
4.674824	384.168491	5.462669
4.542204	390.894089	5.467674
4.315144	379.864747	5.472678
4.515443	375.576855	5.477683
4.266009	383.418410	5.482688
4.803440	375.005260	5.487693
4.491928	368.819172	5.492698
4.512621	364.056145	5.497702
4.808216	356.880944	5.502707
4.248106	365.855490	5.507712
4.439234	359.473873	5.512717
4.191281	368.269569	5.517722
4.386665	376.545587	5.522726
5.011157	378.841520	5.527731
4.392863	396.988441	5.532736
4.967090	394.222568	5.537741
4.458686	393.285036	5.542746
4.664045	388.365894	5.547750
4.790601	381.491203	5.552755
4.589069	386.143791	5.557760
4.822851	385.486910	5.562765
4.495282	375.650255	5.567770
4.692674	384.881129	5.572774
4.713149	383.964716	5.577779
4.770644	396.028331	5.582784
4.576840	381.777808	5.587789
4.785176	390.735476	5.592794
4.928418	391.355956	5.597798
4.820496	391.358331	5.602803
4.598949	391.960269	5.607808
4.743601	383.090334	5.612813
4.690494	386.857130	5.617818
4.602666	400.382966	5.622822
4.987662	396.213516	5.627827
4.663777	390.227960	5.632832
4.850265	395.673942	5.637837
4.755305	401.618380	5.642842
4.535291	384.070475	5.647846
5.189170	392.045796	5.652851
4.691565	395.211543	5.657856
4.764058	385.991563	5.662861
5.001278	397.392306	5.667866
4.849773	401.712547	5.672870
4.894491	395.722307	5.677875
4.801249	397.624437	5.682880
4.774282	390.885015	5.687885
4.963459	386.661605	5.692890
4.748522	390.199726	5.697894
4.726198	385.380070	5.702899
4.963527	389.901335	5.707904
4.965928	387.111083	5.712909
5.070932	408.893815	5.717914
4.996821	402.274844	5.722918
5.447892	408.156178	5.727923
5.149858	398.496253	5.732928
4.931642	394.211420	5.737933
5.278686	389.506427	5.742938
5.071558	395.122131	5.747942
4.819647	392.804932	5.752947
5.130386	405.535545	5.757952
5.236370	417.039184	5.762957
5.170474	423.076201	5.767962
5.356194	411.460084	5.772966
5.284793	408.409834	5.777971
5.238153	412.770955	5.782976
5.606015	395.392650	5.787981
5.160724	403.074598	5.792986
4.904050	399.979495	5.797990
4.971681	395.407197	5.802995
4.986617	422.549310	5.808000
5.282671	417.557359	5.813005
5.284023	419.874689	5.818010
5.621170	422.651412	5.823014
5.412360	414.347456	5.828019
5.205206	431.034340	5.833024
5.168895	426.780505	5.838029
5.296107	426.906902	5.843034
5.152056	429.206729	5.848038
5.293350	427.982962	5.853043
5.490826	426.854190	5.858048
5.495909	415.044467	5.863053
5.347887	421.600765	5.868058
5.556554	423.663043	5.873062
5.370730	426.259131	5.878067
5.499616	426.408337	5.883072
5.500131	427.434105	5.888077
5.399851	427.848684	5.893082
5.581880	428.540989	5.898086
5.885715	423.433112	5.903091
5.510452	435.651541	5.908096
5.715266	423.565814	5.913101
5.866793	431.140267	5.918106
5.595506	431.318314	5.923110
5.648674	431.872685	5.928115
5.178229	422.983129	5.933120
5.511211	418.800663	5.938125
5.725064	430.433286	5.943130
5.180858	440.249347	5.948134
5.312785	424.758616	5.953139
5.096436	433.792115	5.958144
5.484655	433.055647	5.963149
5.436243	431.469001	5.968154
5.178010	435.850693	5.973158
5.816084	430.523907	5.978163
5.711374	453.958134	5.983168
5.717364	463.636819	5.988173
5.428504	459.422146	5.993178
5.303869	465.080773	5.998182
5.457859	457.251554	6.003187
5.622398	463.499118	6.008192
5.580051	455.119783	6.013197
5.658635	473.124201	6.018202
5.686188	456.367761	6.023206
5.782177	460.473188	6.028211
5.836133	466.068167	6.033216
6.212450	457.146388	6.038221
5.542551	459.623193	6.043226
5.783855	466.437283	6.048230
5.831716	454.565903	6.053235
5.686084	457.662150	6.058240
5.850114	452.528928	6.063245
6.134946	455.747994	6.068250
5.704082	468.748805	6.073254
5.907952	466.247258	6.078259
5.633578	465.985513	6.083264
5.924691	464.964485	6.088269
5.797549	456.993589	6.093274
5.761533	462.045831	6.098278
6.024606	460.339338	6.103283
5.852201	460.990082	6.108288
5.735360	464.912158	6.113293
5.658528	452.981475	6.118298
5.675731	456.224644	6.123302
5.919059	460.451732	6.128307
5.842902	461.889434	6.133312
5.702534	456.849134	6.138317
5.771017	457.541954	6.143322
5.845074	456.824156	6.148326
5.702801	453.550511	6.153331
5.448077	473.880879	6.158336
6.043003	459.743225	6.163341
5.778320	458.067813	6.168346
5.709870	463.497053	6.173350
5.780258	459.065457	6.178355
5.751799	456.665544	6.183360
5.630424	448.110444	6.188365
5.856166	462.513954	6.193370
6.081598	459.481626	6.198374
6.262266	446.406701	6.203379
5.654267	455.825569	6.208384
6.149649	451.331535	6.213389
6.262543	451.727460	6.218394
5.872943	458.807210	6.223398
5.981005	452.614593	6.228403
5.700570	441.070854	6.233408
5.530432	445.961657	6.238413
5.933254	440.528523	6.243418
5.875791	455.851441	6.248422
6.056906	459.367339	6.253427
5.506545	443.813833	6.258432
5.772632	441.217164	6.263437
5.905368	457.756946	6.268442
5.667734	454.272250	6.273446
5.952693	450.743219	6.278451
5.869489	454.704030	6.283456
5.748420	423.140730	6.288461
5.753584	436.309586	6.293466
5.438392	433.779185	6.298470
5.893780	433.280131	6.303475
5.807203	454.183105	6.308480
5.782283	456.813083	6.313485
5.730723	461.755228	6.318490
6.104760	464.919796	6.323494
6.111181	440.369874	6.328499
5.788661	440.786848	6.333504
5.778726	432.543739	6.338509
5.901144	440.095384	6.343514
5.971042	431.288286	6.348518
5.881055	419.304358	6.353523
5.928124	431.338154	6.358528
5.693880	437.586300	6.363533
5.639641	430.276401	6.368538
5.384442	426.865449	6.373542
5.641135	429.708249	6.378547
5.602542	427.953154	6.383552
5.717044	442.700198	6.388557
5.744927	445.749418	6.393562
5.862433	455.786238	6.398566
5.982651	452.440407	6.403571
5.632506	446.588802	6.408576
5.339197	453.911116	6.413581
5.889406	450.445884	6.418586
5.703886	461.534145	6.423590
5.984306	460.085829	6.428595
6.047088	457.584415	6.433600
5.794086	457.238931	6.438605
5.959473	450.049393	6.443610
5.342410	443.464293	6.448614
5.815165	447.669248	6.453619
5.598784	465.865554	6.458624
5.408463	457.687364	6.463629
5.833746	463.470083	6.468634
5.696047	463.020009	6.473638
5.743660	446.727796	6.478643
5.556710	464.459203	6.483648
5.530824	456.721568	6.488653
5.947269	454.150955	6.493658
5.515120	480.291408	6.498662
5.688942	449.769472	6.503667
5.943319	468.594657	6.508672
5.789065	462.368830	6.513677
6.104979	457.027794	6.518682
5.927363	463.653818	6.523686
6.325402	456.355487	6.528691
6.069104	466.759134	6.533696
5.923837	461.306470	6.538701
6.122853	447.932839	6.543706
5.762074	442.362880	6.548710
5.575420	430.068269	6.553715
5.678655	438.383424	6.558720
5.468055	448.140906	6.563725
5.585492	452.205889	6.568730
5.602612	466.605304	6.573734
6.079999	453.560755	6.578739
5.992945	466.712912	6.583744
5.932050	456.697961	6.588749
6.016021	455.508132	6.593754
5.575246	464.820446	6.598758
5.861242	457.321417	6.603763
5.932256	447.623951	6.608768
6.078888	440.871209	6.613773
5.970211	443.294530	6.618778
5.491409	438.912756	6.623782
5.880379	430.163917	6.628787
5.493786	436.367392	6.633792
5.604714	432.227637	6.638797
6.019970	428.899251	6.643802
5.738186	437.306447	6.648806
5.658913	429.396417	6.653811
5.874518	445.408099	6.658816
5.630684	451.636921	6.663821
6.104102	453.400227	6.668826
5.929094	446.323869	6.673830
5.791242	432.674832	6.678835
5.767791	425.563472	6.683840
5.598140	430.037368	6.688845
5.637191	416.964759	6.693850
5.382302	441.861892	6.698854
5.919334	456.762382	6.703859
5.905443	459.949622	6.708864
5.997822	459.611778	6.713869
6.233489	454.021679	6.718874
5.424313	442.403818	6.723878
5.514487	431.336021	6.728883
5.933190	453.004229	6.733888
6.149735	458.320762	6.738893
6.085639	451.716492	6.743898
5.784811	441.011246	6.748902
5.598906	422.145832	6.753907
5.547882	436.027783	6.758912
5.583039	428.695120	6.763917
5.785952	421.408137	6.768922
5.808539	443.673746	6.773926
5.836778	442.505460	6.778931
5.852386	435.533652	6.783936
5.345477	437.764305	6.788941
6.044295	448.805759	6.793946
5.698329	461.084282	6.798950
6.290682	459.797711	6.803955
5.789857	445.133986	6.808960
5.632662	427.696010	6.813965
5.919359	439.761441	6.818970
5.401199	439.373157	6.823974
5.771297	442.429751	6.828979
5.987564	463.516012	6.833984
5.551976	432.670894	6.838989
6.352881	441.729062	6.843994
6.298720	451.889551	6.848998
5.844022	433.848715	6.854003
5.429229	444.086653	6.859008
5.636944	436.558248	6.864013
6.068001	435.831767	6.869018
5.522492	431.152720	6.874022
5.899028	431.170039	6.879027
5.551835	440.351346	6.884032
5.653304	445.746481	6.889037
5.938063	424.454183	6.894042
5.526107	441.743577	6.899046
5.695439	436.251263	6.904051
5.268574	437.760635	6.909056
5.890310	455.267822	6.914061
6.129911	452.191522	6.919066
5.878406	450.216781	6.924070
5.832785	438.484478	6.929075
5.930963	436.395224	6.934080
5.706776	440.516462	6.939085
5.884094	440.991616	6.944090
5.762926	439.316758	6.949094
5.746368	443.188516	6.954099
5.925461	429.302321	6.959104
5.648366	442.437423	6.964109
5.998117	427.557480	6.969114
5.692443	428.513291	6.974118
5.845102	424.619102	6.979123
6.132453	430.417105	6.984128
6.079790	429.354828	6.989133
6.211081	431.775388	6.994138
6.004192	437.347955	6.999142
6.092077	431.028259	7.004147
6.172417	442.215918	7.009152
5.884452	438.402534	7.014157
6.010397	438.530621	7.019162
5.691270	430.769638	7.024166
5.954714	411.872398	7.029171
5.740807	422.803429	7.034176
5.531845	426.080218	7.039181
5.719273	423.869076	7.044186
5.546240	433.624977	7.049190
5.752347	431.411141	7.054195
5.831040	432.304024	7.059200
5.721104	440.952153	7.064205
6.070732	430.895520	7.069210
5.896045	446.036740	7.074214
5.953478	434.851328	7.079219
5.882288	438.835504	7.084224
5.545366	431.016493	7.089229
5.944928	431.002580	7.094234
5.572398	425.810054	7.099238
5.565322	426.506974	7.104243
5.824084	437.406665	7.109248
5.981679	430.033049	7.114253
6.121143	427.105698	7.119258
5.697791	423.289239	7.124262
5.625474	423.065135	7.129267
5.386163	423.880640	7.134272
5.558342	425.426270	7.139277
5.573983	433.914340	7.144282
5.488448	435.810761	7.149286
5.470224	427.015565	7.154291
5.650947	435.122081	7.159296
5.571932	438.332805	7.164301
5.924005	442.797437	7.169306
5.787648	436.158253	7.174310
6.092025	431.668068	7.179315
5.877799	442.120979	7.184320
5.808726	435.223346	7.189325
6.030042	434.748866	7.194330
5.615658	437.970421	7.199334
5.797282	421.688842	7.204339
5.811167	434.914165	7.209344
5.392511	440.452474	7.214349
5.373197	427.075184	7.219354
5.330850	436.763911	7.224358
5.699399	427.137155	7.229363
5.534492	442.489457	7.234368
6.039894	460.065697	7.239373
6.355498	461.590489	7.244378
5.969818	443.064785	7.249382
5.987392	443.027084	7.254387
5.971049	445.772550	7.259392
5.638669	430.111016	7.264397
6.022170	441.481402	7.269402
5.636226	435.027997	7.274406
5.936226	429.494755	7.279411
5.841427	440.950893	7.284416
5.628439	438.976201	7.289421
6.141849	430.190125	7.294426
6.017665	441.559171	7.299430
5.838666	433.014590	7.304435
5.646316	434.466559	7.309440
5.447430	435.428400	7.314445
5.856632	440.633769	7.319450
5.466142	435.952582	7.324454
5.688544	430.154743	7.329459
5.863805	431.667406	7.334464
5.956652	435.576625	7.339469
5.911589	433.071333	7.344474
5.628201	437.034935	7.349478
6.217832	432.198879	7.354483
6.081840	433.478258	7.359488
5.534800	435.116997	7.364493
5.894739	433.100011	7.369498
5.781759	438.206892	7.374502
5.737478	433.078505	7.379507
5.841255	441.691809	7.384512
5.831441	436.464297	7.389517
5.970748	433.294869	7.394522
5.666274	436.908372	7.399526
5.530038	441.277107	7.404531
5.777585	439.430821	7.409536
5.668057	444.743325	7.414541
5.844291	438.227399	7.419546
5.625904	445.073447	7.424550
5.806396	435.941645	7.429555
6.096503	445.558271	7.434560
6.010739	442.046111	7.439565
6.002843	430.394497	7.444570
5.833943	445.081139	7.449574
5.432399	435.564181	7.454579
5.694439	431.584532	7.459584
5.408561	442.838533	7.464589
5.651865	433.511569	7.469594
5.591897	443.516544	7.474598
6.053352	437.502207	7.479603
6.087143	438.315201	7.484608
5.792122	436.720671	7.489613
5.917751	431.091150	7.494618
5.777746	446.926011	7.499622
5.860151	436.918074	7.504627
5.963296	449.207804	7.509632
5.816580	433.159238	7.514637
5.882500	436.136071	7.519642
5.544676	441.995564	7.524646
5.722297	438.653173	7.529651
5.765162	436.270285	7.534656
5.727315	442.657934	7.539661
5.576511	422.892894	7.544666
5.777417	431.276847	7.549670
5.945362	438.118931	7.554675
6.075629	436.176008	7.559680
5.480162	436.840926	7.564685
5.776226	427.997638	7.569690
5.678896	436.573240	7.574694
5.741343	441.613347	7.579699
5.732679	429.527181	7.584704
5.775277	435.063846	7.589709
5.816899	436.481687	7.594714
5.672827	437.214763	7.599718
5.357498	426.897964	7.604723
5.443307	442.589941	7.609728
5.544205	441.495380	7.614733
5.630937	435.642416	7.619738
5.825459	446.184841	7.624742
6.068311	442.499100	7.629747
6.119601	436.305217	7.634752
5.621977	447.332086	7.639757
6.047466	438.252234	7.644762
5.720430	435.279148	7.649766
5.785924	433.786344	7.654771
5.598953	432.363477	7.659776
5.839510	444.626746	7.664781
6.072048	436.421699	7.669786
5.632620	438.577272	7.674790
5.832414	434.896773	7.679795
5.897676	429.276242	7.684800
5.629353	433.598138	7.689805
5.626599	435.420995	7.694810
5.598995	432.204962	7.699814
5.741570	445.987151	7.704819
5.895115	438.353749	7.709824
5.567249	433.760968	7.714829
5.930971	438.164776	7.719834
5.728999	438.845661	7.724838
5.685716	431.084770	7.729843
5.688399	440.179450	7.734848
5.913696	447.902036	7.739853
5.810759	437.951957	7.744858
5.835511	439.989975	7.749862
5.875380	453.498406	7.754867
5.663959	435.559527	7.759872
5.605139	435.031404	7.764877
5.942855	439.186161	7.769882
5.741453	440.921980	7.774886
5.819623	445.323848	7.779891
5.784889	439.320676	7.784896
5.573932	443.862174	7.789901
6.328479	456.164817	7.794906
6.097167	445.179144	7.799910
5.595046	437.437843	7.804915
5.893932	442.704952	7.809920
5.675676	448.712009	7.814925
5.926189	436.617635	7.819930
5.693720	441.614630	7.824934
5.652888	436.216636	7.829939
5.924536	445.501474	7.834944
5.844167	445.805820	7.839949
5.667370	441.119702	7.844954
5.504618	442.175708	7.849958
5.600954	443.035389	7.854963
5.910758	432.560326	7.859968
5.952176	442.122845	7.864973
5.974072	447.369433	7.869978
5.931270	447.034297	7.874982
5.850049	428.164598	7.879987
5.946495	437.332768	7.884992
5.977847	444.400068	7.889997
6.019079	438.895281	7.895002
5.767902	454.170497	7.900006
5.841628	434.768485	7.905011
5.845248	436.045905	7.910016
5.838367	438.844757	7.915021
5.882438	435.754996	7.920026
5.757168	443.812738	7.925030
5.837089	446.841322	7.930035
5.761131	436.146766	7.935040
5.753185	447.754594	7.940045
5.756414	443.069209	7.945050
6.117442	434.767261	7.950054
5.739872	444.405435	7.955059
5.487026	436.309313	7.960064
5.957410	439.470285	7.965069
5.824697	438.180811	7.970074
5.787918	430.639934	7.975078
5.958435	437.262379	7.980083
6.094628	435.453833	7.985088
6.068577	440.915816	7.990093
6.116450	436.861557	7.995098
6.028310	430.552699	8.000102
5.451671	406.209189	8.005107
5.510953	418.284069	8.010112
5.724934	441.777549	8.015130
5.748228	436.359916	8.020147
6.049982	440.904969	8.025165
5.999318	444.043220	8.030182
5.593980	429.895240	8.035200
5.818196	443.155787	8.040218
6.029134	432.998104	8.045235
5.675132	436.755555	8.050253
5.782083	441.897642	8.055270
6.027455	435.702816	8.060288
6.024870	425.479266	8.065306
5.898045	410.209129	8.070323
5.346552	418.479750	8.075341
5.645082	432.691875	8.080358
6.014754	441.820693	8.085376
5.646338	441.900894	8.090394
5.928133	441.759590	8.095411
5.936889	450.873960	8.100429
5.927410	441.527928	8.105446
5.864649	445.610891	8.110464
5.885571	443.628355	8.115482
5.705923	443.326056	8.120499
5.961527	436.300188	8.125517
5.636801	432.222770	8.130534
6.087611	439.458853	8.135552
5.955792	448.500115	8.140570
5.939272	441.209536	8.145587
5.873824	438.200648	8.150605
6.096270	447.925037	8.155622
6.054819	441.887133	8.160640
5.860045	444.886143	8.165658
5.577498	441.649703	8.170675
5.608645	434.540187	8.175693
5.669184	448.284285	8.180710
5.848317	440.226096	8.185728
5.550336	439.641547	8.190746
5.629121	452.532026	8.195763
6.035762	438.977846	8.200781
5.749344	439.851510	8.205798
5.833757	446.447705	8.210816
5.868280	459.421177	8.215834
6.008940	465.160133	8.220851
5.881162	471.747123	8.225869
6.059322	472.498550	8.230886
6.248791	459.465278	8.235904
6.233120	471.620754	8.240922
5.913726	458.027914	8.245939
6.090184	455.457487	8.250957
5.897775	459.818027	8.255974
6.268957	456.611118	8.260992
6.037335	458.823770	8.266010
6.307855	449.931748	8.271027
6.073541	436.927003	8.276045
5.755071	440.114922	8.281062
6.076675	437.549640	8.286080
5.874760	452.005968	8.291098
6.164657	466.382804	8.296115
6.069899	466.955659	8.301133
6.263732	468.041629	8.306150
6.256155	453.261183	8.311168
5.873463	447.223284	8.316186
5.731324	448.936603	8.321203
6.167854	458.352646	8.326221
5.860723	465.411896	8.331238
5.978560	466.818333	8.336256
5.967223	471.769688	8.341274
5.886251	471.868710	8.346291
6.454561	465.339855	8.351309
5.932849	476.327749	8.356326
6.150360	470.882141	8.361344
6.396197	471.798527	8.366362
6.133914	482.512007	8.371379
6.516341	464.500438	8.376397
6.027283	474.176123	8.381414
6.279272	478.370235	8.386432
6.268781	469.918751	8.391450
6.368073	477.575762	8.396467
6.347822	477.373964	8.401485
6.428012	474.740424	8.406502
6.020040	461.233366	8.411520
6.063535	467.470858	8.416538
5.879892	475.293694	8.421555
5.963583	468.472070	8.426573
5.954020	478.868840	8.431590
6.094060	468.163618	8.436608
6.166370	463.116143	8.441626
6.374832	473.773667	8.446643
6.372914	470.673680	8.451661
6.351812	473.993036	8.456678
6.528778	478.627901	8.461696
6.346316	477.325194	8.466714
6.206979	474.473164	8.471731
6.400048	474.484289	8.476749
5.988117	483.244077	8.481766
6.175701	470.034865	8.486784
6.232957	479.504448	8.491802
5.878452	481.792517	8.496819
6.427423	474.262536	8.501837
5.936914	480.236977	8.506854
6.128735	469.858559	8.511872
6.351976	477.899824	8.516890
6.215367	479.048669	8.521907
6.479186	485.572033	8.526925
6.244383	479.528477	8.531942
6.398949	474.403539	8.536960
6.224925	476.743064	8.541978
5.909058	476.305336	8.546995
6.213624	472.284705	8.552013
6.284392	478.503228	8.557030
6.482713	482.837974	8.562048
6.470117	487.941577	8.567066
6.483657	480.558728	8.572083
6.282906	477.462864	8.577101
6.283246	482.103597	8.582119
6.432380	490.474076	8.587136
6.468844	480.252204	8.592154
6.139582	475.230939	8.597171
6.515639	489.836913	8.602189
6.356013	505.126186	8.607207
6.662368	496.163465	8.612224
6.528507	491.073493	8.617242
6.352680	487.851389	8.622259
6.406142	476.755533	8.627277
6.093283	484.678255	8.632295
6.467082	496.803238	8.637312
6.198919	501.754043	8.642330
6.317984	507.200287	8.647347
6.506593	509.185362	8.652365
6.456102	510.466010	8.657383
6.309638	503.899093	8.662400
6.717860	493.851848	8.667418
6.501573	511.424919	8.672435
6.476635	498.548970	8.677453
6.366245	513.396740	8.682471
6.591069	503.410598	8.687488
6.733287	505.514241	8.692506
6.713542	512.200300	8.697523
6.660002	503.109984	8.702541
6.409063	506.202719	8.707559
6.630975	509.081415	8.712576
6.749439	511.133681	8.717594
6.292726	510.713324	8.722611
6.472716	508.533169	8.727629
6.703477	519.694120	8.732647
6.695160	515.602867	8.737664
6.688517	503.075885	8.742682
6.391593	504.236958	8.747699
6.653053	508.115897	8.752717
6.626298	500.864178	8.757735
6.194602	504.802560	8.762752
6.714532	510.337054	8.767770
6.563044	499.103336	8.772787
6.790083	497.243390	8.777805
6.601481	513.057922	8.782823
6.580544	512.459665	8.787840
6.600713	512.734552	8.792858
6.521779	521.387569	8.797875
6.779809	507.817346	8.802893
6.533221	510.060228	8.807911
6.395230	512.344404	8.812928
6.448547	511.993075	8.817946
6.157218	509.781481	8.822963
6.673339	510.880617	8.827981
6.576438	509.915761	8.832999
6.704791	506.394124	8.838016
6.601519	509.978295	8.843034
6.646647	509.275931	8.848051
6.817587	503.904530	8.853069
6.514100	509.108072	8.858087
6.427932	511.019880	8.863104
6.523655	502.394560	8.868122
6.359106	504.888789	8.873139
6.960682	516.376467	8.878157
6.700811	516.098249	8.883175
6.586952	514.831731	8.888192
7.134855	518.174558	8.893210
6.576892	517.902994	8.898227
6.831687	504.609432	8.903245
6.830172	502.970584	8.908263
6.651407	498.617406	8.913280
6.962341	514.453006	8.918298
6.921760	504.865670	8.923315
7.127801	510.102602	8.928333
6.859330	512.328239	8.933351
6.890084	506.611576	8.938368
6.794659	502.134312	8.943386
6.487179	506.690518	8.948403
6.734177	506.167742	8.953421
6.537524	504.995206	8.958439
6.323097	515.604462	8.963456
6.978847	517.572661	8.968474
6.921857	532.847361	8.973491
7.148707	530.637318	8.978509
7.152148	525.477410	8.983527
6.809170	517.792806	8.988544
6.895858	497.657785	8.993562
6.896138	513.714964	8.998579
6.398439	511.921942	9.003597
6.851041	518.837361	9.008615
6.926617	528.617660	9.013632
6.997631	542.598350	9.018650
6.759041	541.653758	9.023667
7.245629	540.615205	9.028685
7.048862	530.205511	9.033703
6.734329	509.722988	9.038720
7.248747	513.405334	9.043738
6.739868	524.245109	9.048755
7.149497	508.397935	9.053773
6.974885	503.971840	9.058791
6.859222	507.831918	9.063808
7.029591	494.074267	9.068826
6.763055	507.084937	9.073843
6.736315	511.450882	9.078861
6.798367	511.899911	9.083879
7.033488	537.664909	9.088896
7.231565	541.572241	9.093914
7.183503	544.116207	9.098931
6.952364	533.635830	9.103949
6.876441	516.833768	9.108967
6.646104	523.957995	9.113984
6.923509	533.181529	9.119002
6.839616	542.489278	9.124019
7.277150	529.975860	9.129037
6.976473	531.878248	9.134055
6.957494	537.722436	9.139072
7.313119	528.107592	9.144090
7.077725	544.326953	9.149107
7.286119	531.964665	9.154125
7.506466	538.491791	9.159143
7.449191	533.146876	9.164160
7.166503	512.896044	9.169178
6.733746	516.526105	9.174195
6.982970	503.380285	9.179213
7.236856	512.676773	9.184231
6.805688	516.770058	9.189248
6.981298	511.178341	9.194266
7.370483	539.866090	9.199283
7.381904	527.877133	9.204301
7.419925	504.612408	9.209319
6.854145	514.747062	9.214336
6.748278	509.665349	9.219354
7.178560	522.012958	9.224371
7.192416	531.373529	9.229389
7.458739	530.596823	9.234407
7.189793	538.327018	9.239424
7.180021	513.634942	9.244442
7.187656	515.836304	9.249459
7.027227	514.160836	9.254477
7.231575	513.351763	9.259495
7.234621	533.828456	9.264512
7.355259	518.074593	9.269530
7.511850	518.016860	9.274547
6.850268	503.778903	9.279565
7.097794	505.007940	9.284583
6.898455	525.128777	9.289600
7.267628	531.506922	9.294618
7.261115	531.860612	9.299635
7.104881	532.282048	9.304653
7.087259	536.867904	9.309671
6.760303	539.834163	9.314688
7.004264	535.460514	9.319706
6.937689	548.192555	9.324723
6.787310	537.510284	9.329741
7.422856	537.719589	9.334759
7.011271	544.675591	9.339776
7.347192	541.471442	9.344794
7.423392	566.094978	9.349811
7.434335	549.887554	9.354829
7.566072	539.005443	9.359847
7.223837	545.823043	9.364864
7.310272	534.366356	9.369882
7.138474	545.769998	9.374899
7.375147	559.297527	9.379917
7.737298	557.976056	9.384935
7.282728	563.077936	9.389952
7.432815	550.227930	9.394970
7.132817	549.826153	9.399987
7.236089	554.004123	9.405005
7.295450	567.779815	9.410023
7.593348	575.777598	9.415040
7.744091	571.026512	9.420058
7.491339	559.959256	9.425075
7.404682	555.114954	9.430093
7.520915	538.221185	9.435111
7.303644	537.187851	9.440128
7.087426	543.968880	9.445146
7.657358	557.794608	9.450163
7.792962	549.665422	9.455181
7.894166	540.870803	9.460199
7.667777	542.807264	9.465216
7.567995	538.551728	9.470234
7.454531	543.385858	9.475251
7.477222	541.113803	9.480269
7.495874	545.282335	9.485287
6.959749	545.729847	9.490304
7.402896	536.193822	9.495322
7.485850	535.912383	9.500339
7.437769	552.518526	9.505357
7.339894	545.693120	9.510375
7.186782	544.095360	9.515392
7.223074	573.208737	9.520410
7.253599	573.260994	9.525427
7.667286	576.148159	9.530445
7.975002	571.823598	9.535463
7.757571	581.877210	9.540480
7.446133	570.418644	9.545498
7.890914	572.602584	9.550515
7.465820	576.262291	9.555533
7.825587	567.708826	9.560551
7.530708	572.466963	9.565568
7.732539	576.907138	9.570586
7.762994	564.628058	9.575603
7.555565	564.471460	9.580621
7.695798	548.530605	9.585639
7.679844	556.012251	9.590656
7.826055	557.329674	9.595674
7.659477	553.328135	9.600691
7.301208	542.495510	9.605709
7.719820	558.333829	9.610727
7.834292	571.698334	9.615744
7.668138	540.899546	9.620762
7.610417	537.824315	9.625779
7.430471	554.875591	9.630797
7.805731	555.222183	9.635815
7.543450	561.943818	9.640832
7.777593	569.256607	9.645850
7.841522	564.150062	9.650867
7.876390	573.571051	9.655885
7.846141	566.031749	9.660903
7.648954	569.813306	9.665920
7.930348	569.167742	9.670938
7.875191	560.133750	9.675955
7.624882	556.530123	9.680973
7.803901	546.093545	9.685991
7.991140	549.678819	9.691008
7.343093	538.532053	9.696026
7.743814	549.103440	9.701043
7.744185	566.776469	9.706061
7.766092	569.360835	9.711079
7.899409	575.542688	9.716096
7.679047	576.801327	9.721114
7.632686	571.025548	9.726131
7.613186	566.017813	9.731149
7.717717	561.750155	9.736167
8.143708	573.585824	9.741184
7.616963	563.964545	9.746202
7.728840	561.166141	9.751219
7.621998	567.767819	9.756237
8.230580	560.831464	9.761255
7.971913	566.381286	9.766272
7.917379	570.278118	9.771290
7.632483	564.217025	9.776307
7.736446	576.279895	9.781325
8.006442	571.693610	9.786343
8.006371	571.854937	9.791360
8.161099	567.763393	9.796378
7.894581	561.764605	9.801395
7.619581	566.226994	9.806413
7.903549	562.957327	9.811431
7.643202	566.427241	9.816448
7.628800	567.888999	9.821466
7.444103	565.505574	9.826483
7.623525	580.296265	9.831501
7.853884	587.761330	9.836519
7.885669	592.444430	9.841536
7.899958	601.787850	9.846554
8.381578	595.682140	9.851571
7.883095	602.565342	9.856589
8.084778	597.502347	9.861607
7.985972	601.496642	9.866624
7.562770	598.620845	9.871642
8.063722	590.971899	9.876659
7.632470	603.164274	9.881677
8.265344	603.120825	9.886695
8.448810	597.111622	9.891712
7.958756	596.168533	9.896730
8.223743	586.891795	9.901747
8.177927	597.673989	9.906765
8.176372	601.520154	9.911783
8.031571	589.401289	9.916800
8.412466	605.135676	9.921818
8.283867	599.886365	9.926835
8.223527	597.588663	9.931853
8.315940	601.794714	9.936871
8.496251	597.217142	9.941888
7.977727	591.087484	9.946906
7.984966	574.591925	9.951923
8.263139	575.318661	9.956941
7.984656	563.206952	9.961959
8.104161	583.459487	9.966976
8.233760	591.606032	9.971994
8.408671	588.671345	9.977011
7.926649	600.437649	9.982029
8.515773	590.610592	9.987047
8.469172	582.647299	9.992064
8.004953	581.792540	9.997082
8.231007	573.134424	10.002099
8.128833	587.015355	10.007117
8.083913	584.160592	10.012135
8.255033	586.492888	10.017152
8.190060	596.956758	10.022170
8.362366	598.447789	10.027187
8.408613	602.589339	10.032205
8.490633	598.299904	10.037223
8.469416	580.902727	10.042240
8.622964	584.500466	10.047258
8.303189	579.771830	10.052275
7.848985	574.746578	10.057293
7.429760	574.298080	10.062311
8.102565	593.492163	10.067328
8.120988	597.688398	10.072346
8.397745	602.954218	10.077363
8.192426	602.629392	10.082381
8.043356	603.199813	10.087399
8.580804	601.177752	10.092416
8.254165	604.457391	10.097434
8.518214	595.645375	10.102451
7.813381	603.713725	10.107469
8.002766	589.374814	10.112487
8.504719	603.814550	10.117504
8.240756	604.310768	10.122522
8.350464	591.242446	10.127539
8.705215	612.300853	10.132557
8.193530	610.957679	10.137575
8.829434	600.106455	10.142592
8.296078	604.964335	10.147610
8.390160	598.030525	10.152627
8.143259	606.643744	10.157645
8.421672	614.344533	10.162663
8.809087	630.406346	10.167680
8.759141	620.813203	10.172698
8.633754	603.201766	10.177715
8.543069	607.968286	10.182733
8.640631	607.084552	10.187751
8.649157	600.917288	10.192768
8.469387	600.955784	10.197786
8.611691	602.132350	10.202803
8.549200	608.198869	10.207821
8.638612	609.454733	10.212839
8.404347	611.682210	10.217856
8.129217	601.826549	10.222874
8.678556	595.983314	10.227891
8.563805	604.518897	10.232909
8.330708	598.757632	10.237927
8.455419	607.453504	10.242944
8.626290	627.704694	10.247962
9.025158	622.108515	10.252979
8.716130	613.534769	10.257997
8.328459	602.114756	10.263015
8.485692	601.564399	10.268032
8.529230	620.336531	10.273050
8.786429	639.607030	10.278067
9.125007	630.468566	10.283085
8.545458	604.362932	10.288103
8.788214	594.801634	10.293120
8.436565	597.059824	10.298138
8.239022	612.544506	10.303155
8.162785	620.140062	10.308173
8.850399	624.076630	10.313191
8.657157	618.849018	10.318208
8.879141	631.031867	10.323226
8.924616	627.413291	10.328243
8.966557	625.002047	10.333261
8.841201	623.928622	10.338279
8.889535	628.258182	10.343296
8.693923	627.896424	10.348314
8.542646	619.530415	10.353331
8.801571	637.939677	10.358349
8.479767	635.966421	10.363367
8.958817	623.548999	10.368384
8.724464	631.809244	10.373402
8.625025	631.498803	10.378419
8.802690	637.629366	10.383437
8.632766	642.365102	10.388455
8.888096	631.455219	10.393472
8.606564	638.475286	10.398490
8.694714	634.627358	10.403507
8.375142	633.737277	10.408525
8.420196	636.495746	10.413543
8.816650	629.932538	10.418560
8.915416	643.970335	10.423578
8.727538	644.649906	10.428595
8.848109	640.640055	10.433613
8.811350	660.665909	10.438631
9.288853	666.701960	10.443648
9.386553	650.937188	10.448666
8.995424	640.607069	10.453683
8.987586	639.299500	10.458701
8.908459	646.807277	10.463719
9.115788	637.497625	10.468736
8.895429	640.342861	10.473754
8.831874	637.494415	10.478771
9.054817	639.613373	10.483789
8.661280	634.367685	10.488807
8.993165	626.917296	10.493824
9.049729	634.246965	10.498842
8.853076	620.152789	10.503859
9.104662	627.035446	10.508877
8.996058	631.202496	10.513895
9.008002	628.469699	10.518912
9.124112	637.279783	10.523930
8.873340	630.865160	10.528947
8.913303	640.381785	10.533965
8.571423	652.398930	10.538983
8.904664	650.069536	10.544000
9.140501	654.659988	10.549018
9.348331	650.492534	10.554035
9.598221	650.537175	10.559053
9.123759	651.482075	10.564071
9.390742	643.330636	10.569088
9.118153	636.320425	10.574106
8.802164	626.013521	10.579123
9.203221	641.342725	10.584141
9.025618	654.204794	10.589159
9.370306	659.890030	10.594176
9.261499	659.260138	10.599194
9.062648	649.453836	10.604211
9.200358	654.243835	10.609229
8.649632	663.250239	10.614247
9.207545	653.827532	10.619264
9.312938	654.475760	10.624282
9.078809	655.378286	10.629299
9.730469	656.542517	10.634317
9.298896	664.430137	10.639335
9.568011	650.337587	10.644352
9.525862	645.994658	10.649370
9.390722	643.638064	10.654387
9.487138	631.891425	10.659405
9.143082	630.298839	10.664423
9.188143	626.350083	10.669440
9.231957	626.841098	10.674458
8.758201	630.227420	10.679475
9.376423	632.772688	10.684493
9.220251	646.175390	10.689511
9.440145	652.434977	10.694528
9.141713	652.206722	10.699546
9.200114	650.851993	10.704563
9.368370	659.118636	10.709581
9.628194	658.305899	10.714599
9.495799	649.556219	10.719616
9.741472	661.413293	10.724634
9.623815	642.615138	10.729651
9.516066	629.695591	10.734669
9.262844	642.463180	10.739687
9.246078	631.557129	10.744704
9.397448	631.120119	10.749722
9.322175	637.095867	10.754739
9.581920	639.751450	10.759757
9.281391	642.221037	10.764775
9.589535	651.604883	10.769792
9.671629	644.654041	10.774810
9.308705	649.480620	10.779827
9.644691	639.486352	10.784845
9.167831	638.162513	10.789863
9.357895	651.662892	10.794880
9.357241	657.970146	10.799898
9.144961	655.593038	10.804915
9.284803	663.371760	10.809933
9.210214	658.741923	10.814951
9.224993	665.588058	10.819968
9.766892	651.406538	10.824986
9.477769	664.183719	10.830003
9.421974	658.827592	10.835021
9.345592	653.565107	10.840039
9.285913	660.950606	10.845056
9.585711	659.216975	10.850074
9.470879	655.116915	10.855091
9.352226	669.724615	10.860109
9.509514	692.536194	10.865127
9.730908	686.476308	10.870144
10.153806	690.885100	10.875162
9.853234	687.039304	10.880179
9.804176	663.181565	10.885197
9.514479	668.855033	10.890215
9.794573	664.442608	10.895232
9.527469	662.040116	10.900250
9.512059	657.532068	10.905267
9.637369	662.770093	10.910285
9.588142	682.069340	10.915303
9.733630	689.269008	10.920320
10.127253	686.840672	10.925338
9.478018	685.138013	10.930355
10.066865	683.392628	10.935373
10.078823	677.129903	10.940391
9.746424	661.541786	10.945408
9.701543	661.338250	10.950426
9.423627	664.632779	10.955443
9.640037	664.688365	10.960461
9.743481	686.311628	10.965479
9.966318	693.695721	10.970496
9.986713	690.757128	10.975514
9.942968	692.181530	10.980531
9.650435	677.909975	10.985549
9.639138	675.464026	10.990567
9.890415	702.115529	10.995584
9.956035	692.534241	11.000602
10.040861	701.697889	11.005619
10.094086	693.512569	11.010637
9.692972	685.391513	11.015655
9.705653	686.645204	11.020672
10.123881	686.965510	11.025690
9.768562	695.578293	11.030707
10.040262	696.070718	11.035725
9.950142	700.139278	11.040743
9.756856	699.442455	11.045760
10.022153	695.281237	11.050778
9.917445	700.082183	11.055795
9.868192	690.395003	11.060813
9.707101	689.242160	11.065831
9.775091	696.482684	11.070848
10.203630	697.288593	11.075866
9.841012	697.344316	11.080883
9.592367	701.101640	11.085901
9.480715	691.227073	11.090919
9.653192	706.015982	11.095936
10.072402	700.223341	11.100954
9.971880	711.600959	11.105971
10.260295	723.128540	11.110989
10.050887	709.698859	11.116007
10.193455	700.750197	11.121024
10.070144	703.914381	11.126042
9.915930	704.621357	11.131059
10.115181	718.875347	11.136077
9.999972	726.987435	11.141095
10.490573	727.217450	11.146112
10.520257	719.934061	11.151130
9.998261	709.805606	11.156147
9.893815	692.360554	11.161165
10.210727	703.134345	11.166183
10.257999	706.520979	11.171200
10.373403	703.642947	11.176218
10.065035	695.181818	11.181235
9.878643	700.944799	11.186253
10.249422	708.887211	11.191271
10.386639	721.442240	11.196288
10.450317	720.703737	11.201306
10.076560	712.437129	11.206323
10.297778	728.336095	11.211341
10.537555	723.610988	11.216359
10.362664	711.946321	11.221376
10.330004	691.311777	11.226394
10.439396	700.096339	11.231411
10.390988	697.262305	11.236429
9.892804	703.206118	11.241447
10.166960	707.791730	11.246464
10.533700	713.082179	11.251482
10.117646	727.435991	11.256499
9.964486	724.632056	11.261517
10.273820	720.732498	11.266535
10.273619	729.701986	11.271552
10.297651	726.357449	11.276570
10.327969	725.927649	11.281587
10.168686	727.774810	11.286605
10.516162	721.266991	11.291623
10.525518	718.947026	11.296640
10.462356	726.665450	11.301658
10.091906	725.189791	11.306675
10.231234	718.278858	11.311693
10.596742	720.174306	11.316711
10.453271	735.383298	11.321728
10.772346	725.816096	11.326746
10.763147	731.833117	11.331763
10.609402	735.018574	11.336781
11.110584	726.874442	11.341799
10.699910	730.044692	11.346816
11.025972	721.853532	11.351834
10.473658	711.728512	11.356851
10.409219	703.519235	11.361869
10.732994	712.348182	11.366887
10.380527	717.435208	11.371904
10.554641	709.491859	11.376922
10.769711	733.590253	11.381939
10.599295	735.240179	11.386957
10.699179	724.619648	11.391975
10.904362	720.956255	11.396992
10.400481	706.981853	11.402010
10.644744	709.813496	11.407027
10.403274	715.137935	11.412045
10.689181	714.838304	11.417063
10.497596	724.959967	11.422080
10.426916	727.642715	11.427098
10.591070	728.889091	11.432115
10.453437	730.947004	11.437133
10.568873	725.788398	11.442151
10.265859	733.934380	11.447168
10.518357	734.336297	11.452186
10.665522	728.309425	11.457203
10.585126	722.907351	11.462221
10.775794	721.938552	11.467239
10.501957	728.938592	11.472256
10.669049	722.702859	11.477274
10.691173	728.947531	11.482291
10.792434	741.597281	11.487309
11.092911	742.667320	11.492327
10.577422	732.883475	11.497344
10.711119	723.820736	11.502362
10.971363	740.554834	11.507379
10.822511	744.459228	11.512397
11.017309	746.642781	11.517415
10.756010	740.226408	11.522432
10.813193	735.773158	11.527450
11.125738	750.614932	11.532467
10.650703	747.477744	11.537485
11.227399	742.459498	11.542503
11.082465	731.496620	11.547520
10.933825	728.220473	11.552538
10.720776	729.716451	11.557555
11.036155	734.841217	11.562573
11.090217	720.124624	11.567591
11.131392	719.991298	11.572608
10.942963	725.329510	11.577626
10.655795	724.777506	11.582643
10.603882	727.891025	11.587661
10.753418	739.485361	11.592679
10.815918	743.722275	11.597696
10.994056	744.833099	11.602714
11.094832	752.637414	11.607731
11.012260	755.795172	11.612749
11.176106	741.719738	11.617767
10.982264	755.100518	11.622784
11.226160	760.243501	11.627802
11.413087	752.344559	11.632819
11.013641	766.570786	11.637837
11.081642	755.136466	11.642855
11.335006	756.620120	11.647872
11.400145	747.768067	11.652890
11.393084	756.606152	11.657907
11.082128	754.774760	11.662925
11.515946	745.832654	11.667943
11.239985	725.585645	11.672960
10.799873	728.225430	11.677978
11.288570	730.546694	11.682995
10.917770	743.315100	11.688013
11.310794	750.408449	11.693031
11.555840	753.331292	11.698048
11.383713	746.728264	11.703066
11.459759	731.238884	11.708083
11.175619	726.414567	11.713101
11.259726	712.747143	11.718119
10.739819	727.200286	11.723136
11.044618	737.828199	11.728154
11.305634	754.032758	11.733171
10.868155	755.232723	11.738189
11.018596	753.175701	11.743207
11.140036	749.287604	11.748224
11.239072	742.503276	11.753242
11.159246	756.172439	11.758259
10.899336	762.802350	11.763277
11.038449	746.968639	11.768295
11.309974	759.530337	11.773312
11.630772	778.134621	11.778330
11.630441	769.281272	11.783347
11.647780	774.801104	11.788365
11.568097	753.804337	11.793383
11.008730	761.698266	11.798400
10.938268	769.155566	11.803418
11.446062	763.912229	11.808435
11.045697	772.355467	11.813453
11.532058	768.647465	11.818471
11.283942	776.065833	11.823488
11.634281	787.550854	11.828506
11.666574	779.025903	11.833523
11.375800	778.830133	11.838541
11.396983	775.974251	11.843559
11.673943	777.749818	11.848576
11.380082	781.116579	11.853594
11.776434	783.329317	11.858611
11.848140	777.605786	11.863629
12.076860	774.165219	11.868647
12.008460	777.859021	11.873664
11.724439	772.694282	11.878682
12.050143	771.746463	11.883699
11.409632	760.324326	11.888717
11.432450	761.529506	11.893735
11.570448	770.031580	11.898752
11.547287	778.544742	11.903770
11.890646	771.101639	11.908787
11.869248	776.463633	11.913805
12.061746	766.664419	11.918823
11.960979	759.430715	11.923840
11.431398	752.495591	11.928858
11.354613	745.927289	11.933875
11.382625	766.536163	11.938893
11.411522	755.021609	11.943911
11.888053	766.848880	11.948928
11.517103	773.621826	11.953946
12.156733	767.828160	11.958963
11.772442	773.442214	11.963981
11.748947	768.106986	11.968999
11.931335	774.423499	11.974016
12.126162	783.263170	11.979034
12.128161	770.080434	11.984051
11.915416	772.070465	11.989069
12.088716	772.858629	11.994087
11.800660	759.134874	11.999104
11.381904	770.401083	12.004122
11.872354	771.026226	12.009139
11.937946	780.148127	12.014157
11.797527	770.954709	12.019175
11.868149	765.437818	12.024192
11.716309	771.635582	12.029210
11.872460	770.017688	12.034227
11.442441	780.646911	12.039245
11.820478	764.040570	12.044263
11.906034	777.522117	12.049280
11.649612	789.549749	12.054298
11.736160	771.864716	12.059315
11.593441	789.281583	12.064333
11.536401	811.168113	12.069351
12.016243	803.783428	12.074368
12.127215	798.851084	12.079386
12.360710	805.242318	12.084403
12.011029	804.030689	12.089421
12.103118	802.828715	12.094439
12.236323	804.719265	12.099456
11.973319	805.030128	12.104474
12.089481	807.066480	12.109491
12.179897	808.559354	12.114509
12.116665	794.694102	12.119527
12.192309	801.503965	12.124544
11.993445	811.008009	12.129562
12.222465	800.735700	12.134579
12.253991	808.522851	12.139597
12.565005	803.360436	12.144615
12.558041	801.844973	12.149632
12.268507	809.657432	12.154650
12.342774	797.022468	12.159667
12.012135	813.368755	12.164685
11.626418	811.576774	12.169703
11.905325	804.821343	12.174720
11.642996	810.807307	12.179738
11.997629	797.446020	12.184755
12.491388	805.021964	12.189773
12.316892	810.618681	12.194791
12.298758	809.919870	12.199808
11.995990	804.930134	12.204826
12.727355	816.601572	12.209843
12.337172	808.175846	12.214861
12.363951	816.138555	12.219879
12.451749	802.619724	12.224896
12.600279	808.084922	12.229914
12.423240	799.352965	12.234931
12.294288	798.782291	12.239949
12.433138	797.223247	12.244967
12.505250	798.857701	12.249984
12.357227	805.013025	12.255002
12.439282	806.416255	12.260019
12.362294	811.956708	12.265037
12.356162	824.172587	12.270055
12.795275	830.177555	12.275072
12.953816	834.669045	12.280090
12.500819	811.849598	12.285107
12.478294	807.915802	12.290125
12.501722	799.106335	12.295143
12.748931	790.620158	12.300160
12.809684	812.017726	12.305178
12.843231	795.692943	12.310195
13.051004	794.966640	12.315213
12.689944	808.600452	12.320231
12.725152	801.718792	12.325248
12.693162	798.888127	12.330266
12.625803	797.814355	12.335283
12.580601	795.225101	12.340301
12.410656	795.042428	12.345319
12.744409	802.634382	12.350336
12.237275	797.570076	12.355354
12.815985	799.076922	12.360371
12.328845	798.484059	12.365389
12.367440	803.855141	12.370407
12.585698	816.746297	12.375424
12.743176	838.797182	12.380442
12.731886	824.219021	12.385459
12.671553	833.232064	12.390477
12.233234	834.105266	12.395495
12.767257	824.534660	12.400512
12.491728	832.178410	12.405530
12.904033	830.318904	12.410547
12.751946	819.346911	12.415565
12.406893	828.185293	12.420583
12.817326	832.989715	12.425600
12.836307	836.660529	12.430618
12.670304	824.604519	12.435635
12.940043	831.741406	12.440653
12.607873	827.758992	12.445671
13.359397	830.581815	12.450688
12.913112	838.419110	12.455706
13.066028	835.005425	12.460723
13.102419	831.116503	12.465741
12.642892	838.284753	12.470759
12.891756	839.094088	12.475776
12.984325	837.644047	12.480794
13.103626	851.671752	12.485811
13.150471	848.050634	12.490829
13.034981	841.914003	12.495847
13.219091	834.936179	12.500864
12.944627	843.996620	12.505882
13.196324	830.306514	12.510899
13.045228	841.275537	12.515917
12.620910	838.637530	12.520935
12.721186	850.709097	12.525952
12.892308	870.587801	12.530970
12.995618	877.105875	12.535987
13.334016	866.815840	12.541005
13.125830	872.899455	12.546023
13.329130	864.598315	12.551040
13.328966	865.219320	12.556058
13.242836	873.765969	12.561075
13.314076	868.748847	12.566093
13.024903	872.662882	12.571111
13.213130	874.598865	12.576128
13.294121	868.364607	12.581146
13.274612	862.252747	12.586163
13.631242	870.431988	12.591181
13.139917	872.667737	12.596199
13.501192	865.515865	12.601216
13.698586	866.960068	12.606234
13.469112	871.646475	12.611251
13.257504	847.348568	12.616269
13.104624	861.979426	12.621287
13.041787	857.562115	12.626304
13.066968	864.755964	12.631322
13.010881	862.710425	12.636339
13.311699	853.222132	12.641357
13.050169	867.246067	12.646375
13.159845	874.165474	12.651392
12.874937	869.864272	12.656410
13.183434	880.955072	12.661427
13.493844	892.339604	12.666445
13.440068	906.888588	12.671463
13.735529	894.352399	12.676480
13.666348	893.646767	12.681498
13.330308	886.913610	12.686515
13.783428	890.359964	12.691533
13.536755	890.323705	12.696551
13.603082	900.406109	12.701568
13.540008	892.519773	12.706586
13.631562	892.449269	12.711603
13.505329	889.829697	12.716621
13.455387	889.160151	12.721639
14.045947	888.667677	12.726656
13.788490	887.585459	12.731674
13.387938	871.741806	12.736691
13.544988	879.131546	12.741709
13.561874	888.209110	12.746727
13.991743	877.444685	12.751744
13.655707	894.149168	12.756762
13.647849	893.509569	12.761779
14.007813	884.677011	12.766797
13.506107	881.907324	12.771815
13.831647	880.414744	12.776832
13.924059	883.031303	12.781850
13.811315	889.957263	12.786867
13.756786	883.637934	12.791885
13.640305	878.204079	12.796903
13.816603	894.068816	12.801920
14.004440	876.661064	12.806938
13.602645	876.894785	12.811955
13.979087	888.229531	12.816973
13.489615	892.759833	12.821991
13.761140	893.845001	12.827008
13.882288	891.517459	12.832026
13.954339	893.246109	12.837043
13.924803	885.262126	12.842061
13.730594	893.930368	12.847079
13.917045	896.166395	12.852096
14.067337	888.916234	12.857114
14.051206	897.302930	12.862131
14.001268	889.608976	12.867149
13.348392	892.763684	12.872167
13.645203	893.174618	12.877184
13.905074	893.734741	12.882202
13.565658	895.465753	12.887219
14.078644	883.484953	12.892237
13.713807	889.442227	12.897255
13.652264	913.684728	12.902272
14.028530	924.169783	12.907290
13.757837	924.005923	12.912307
14.188955	914.061098	12.917325
14.131904	927.988906	12.922343
14.187375	928.045111	12.927360
14.295396	926.310374	12.932378
13.919518	926.188990	12.937395
13.925639	924.303997	12.942413
14.124642	936.071474	12.947431
14.314423	920.982029	12.952448
14.600706	922.353880	12.957466
14.265325	931.686007	12.962483
14.354831	924.830451	12.967501
14.538495	922.677086	12.972519
14.290947	933.056613	12.977536
14.341500	920.310232	12.982554
14.341338	935.440926	12.987571
14.285753	930.243204	12.992589
14.528231	924.463843	12.997607
14.337704	928.828730	13.002624
14.524493	919.549068	13.007642
14.268557	935.300568	13.012659
14.241269	924.866043	13.017677
14.529142	929.572366	13.022695
14.527781	931.847210	13.027712
14.636952	927.572681	13.032730
14.418531	937.838067	13.037747
14.477920	923.187120	13.042765
14.331440	927.320064	13.047783
14.158883	926.467764	13.052800
14.451583	920.829291	13.057818
14.220574	921.939054	13.062835
14.660086	926.548873	13.067853
14.228969	926.869709	13.072871
14.186456	929.297587	13.077888
14.182566	922.326289	13.082906
14.360858	931.183735	13.087923
14.296838	922.657400	13.092941
14.523928	937.003037	13.097959
14.156778	956.351428	13.102976
14.719284	951.478841	13.107994
14.340778	959.165650	13.113011
14.919429	954.393328	13.118029
14.857306	948.095697	13.123047
14.604705	948.427379	13.128064
14.721346	950.697388	13.133082
14.595398	948.282447	13.138099
14.710018	952.020342	13.143117
14.864683	950.424817	13.148135
14.712158	949.841598	13.153152
15.110441	951.532285	13.158170
14.756610	951.815551	13.163187
14.632546	955.318138	13.168205
15.096178	953.527878	13.173223
14.859176	952.871725	13.178240
14.704565	939.181652	13.183258
15.028637	966.072916	13.188275
14.918671	957.784429	13.193293
15.202333	961.216094	13.198311
15.056899	957.703091	13.203328
14.711299	947.587937	13.208346
14.672786	940.764256	13.213363
14.767456	945.224610	13.218381
14.733625	953.315988	13.223399
14.669010	947.444282	13.228416
15.209600	941.969621	13.233434
14.952804	950.730408	13.238451
15.202736	944.821287	13.243469
15.252770	952.000443	13.248487
14.851901	946.838619	13.253504
15.337205	957.667620	13.258522
15.205469	957.164513	13.263539
15.040034	945.360336	13.268557
14.987854	953.023524	13.273575
14.955240	959.111715	13.278592
15.054960	944.595692	13.283610
14.938523	952.012556	13.288627
15.068500	949.546759	13.293645
15.081667	947.194541	13.298663
15.044776	945.887615	13.303680
15.203819	947.069609	13.308698
14.984566	945.995539	13.313715
14.875121	939.628678	13.318733
15.146556	951.697723	13.323751
14.806814	954.716360	13.328768
15.042160	963.093319	13.333786
15.216953	981.718141	13.338803
15.606665	976.142243	13.343821
15.825388	980.202448	13.348839
15.408999	975.906806	13.353856
15.461708	938.203472	13.358874
15.449601	950.061251	13.363891
15.365410	947.695206	13.368909
15.682411	943.994486	13.373927
15.276302	947.250131	13.378944
15.284171	947.023113	13.383962
15.335732	950.612403	13.388979
15.202638	946.104923	13.393997
15.279740	959.160938	13.399015
15.172937	976.700798	13.404032
15.498136	977.166777	13.409050
15.392255	976.563056	13.414067
15.552362	980.598702	13.419085
15.564733	983.280563	13.424103
15.769568	992.115059	13.429120
15.881885	989.773314	13.434138
15.591021	984.280361	13.439155
15.443281	986.493888	13.444173
15.535551	981.672825	13.449191
15.610996	980.971532	13.454208
16.036373	980.370059	13.459226
15.908372	975.162541	13.464243
15.503646	986.049883	13.469261
15.534045	989.167763	13.474279
15.696248	988.114002	13.479296
15.928882	994.541180	13.484314
16.391199	986.455491	13.489331
15.748512	957.252954	13.494349
15.636472	952.105590	13.499367
15.270046	954.723887	13.504384
15.184563	959.419097	13.509402
15.452249	983.547863	13.514419
15.364335	978.847605	13.519437
15.592093	975.915134	13.524455
15.759312	992.780903	13.529472
15.747285	985.538823	13.534490
15.643641	985.054199	13.539507
15.502414	997.974310	13.544525
16.011310	993.474580	13.549543
16.138994	1014.899945	13.554560
16.170759	1007.493558	13.559578
16.130124	994.315216	13.564595
15.720272	984.101030	13.569613
15.857336	982.861005	13.574631
15.806885	989.339391	13.579648
15.871891	993.132535	13.584666
16.194941	1004.031387	13.589683
16.112195	1013.510363	13.594701
16.318264	1008.194289	13.599719
16.129025	1002.311569	13.604736
15.873992	993.726225	13.609754
16.221582	1001.097330	13.614771
15.992978	1016.580563	13.619789
16.487845	1012.925125	13.624807
16.222074	997.961273	13.629824
16.224498	995.776836	13.634842
16.083331	990.103560	13.639859
15.567710	993.258141	13.644877
16.189386	1007.830218	13.649895
16.305323	1014.678096	13.654912
16.461198	1009.976510	13.659930
16.460034	1027.104157	13.664947
16.399606	1014.249879	13.669965
16.634042	1015.077944	13.674983
16.283877	1002.624645	13.680000
16.015028	995.992422	13.685018
16.019001	998.957907	13.690035
16.134260	1007.948628	13.695053
16.318890	1012.787175	13.700071
16.078046	1010.293886	13.705088
16.338656	1001.925928	13.710106
16.522271	1013.885837	13.715123
16.217194	1018.444452	13.720141
16.457636	1011.446316	13.725159
16.379232	1023.118586	13.730176
16.288119	1015.927154	13.735194
16.203124	1011.110282	13.740211
16.294044	1026.037365	13.745229
16.548794	1013.310892	13.750247
16.328252	1023.117808	13.755264
16.456832	1040.633998	13.760282
16.819869	1036.722927	13.765299
16.559696	1046.767766	13.770317
16.686515	1044.623287	13.775335
16.915381	1041.769642	13.780352
16.452132	1030.161146	13.785370
16.703873	1034.114352	13.790387
16.938753	1032.674430	13.795405
16.712298	1015.236677	13.800423
16.488268	1011.509623	13.805440
16.339349	1031.138819	13.810458
16.699706	1041.016649	13.815475
16.411485	1047.626856	13.820493
16.769029	1042.628494	13.825511
16.760751	1047.887940	13.830528
16.650500	1048.162247	13.835546
16.811694	1037.155744	13.840563
16.602216	1043.756283	13.845581
16.944405	1043.045053	13.850599
16.945214	1048.731074	13.855616
16.828326	1044.866739	13.860634
16.924326	1043.803840	13.865651
16.702331	1047.518956	13.870669
16.837064	1043.431969	13.875687
16.610448	1048.726120	13.880704
16.545478	1049.132487	13.885722
16.768850	1048.702264	13.890739
16.662467	1057.789277	13.895757
16.947583	1070.187200	13.900775
17.107751	1072.697433	13.905792
17.089747	1074.671459	13.910810
17.293018	1074.394336	13.915827
17.181444	1073.164887	13.920845
17.140447	1056.068029	13.925863
16.926493	1054.935309	13.930880
16.997196	1071.149808	13.935898
17.011232	1066.045537	13.940915
16.829108	1071.550021	13.945933
17.065860	1071.102826	13.950951
17.040504	1074.645712	13.955968
17.283076	1065.859021	13.960986
17.357747	1073.826939	13.966003
17.189687	1085.295410	13.971021
17.485684	1068.449094	13.976039
17.541384	1074.699183	13.981056
17.160561	1073.127681	13.986074
17.379320	1066.769511	13.991091
17.529211	1079.109881	13.996109
17.411825	1059.891459	14.001127
17.202530	1077.695475	14.006144
16.902232	1072.779542	14.011162
17.306430	1063.282597	14.016179
17.063663	1069.441875	14.021197
17.417526	1072.415092	14.026215
17.373400	1066.439283	14.031232
17.450602	1072.806270	14.036250
17.271150	1075.379123	14.041267
16.803491	1067.898969	14.046285
17.547592	1078.486699	14.051303
17.722598	1091.051236	14.056320
17.522667	1086.853036	14.061338
17.817858	1095.470824	14.066355
17.319137	1087.045757	14.071373
17.679475	1086.428951	14.076391
17.937757	1098.976189	14.081408
17.485555	1084.181326	14.086426
17.430560	1081.436089	14.091443
17.820218	1099.873801	14.096461
17.973186	1093.677056	14.101479
17.935520	1082.539042	14.106496
17.482564	1081.167027	14.111514
17.480015	1073.439563	14.116531
17.648510	1095.710611	14.121549
17.755029	1098.487741	14.126567
18.039679	1112.870086	14.131584
17.870948	1106.534209	14.136602
17.860036	1095.210102	14.141619
17.845732	1090.621050	14.146637
17.784404	1086.944340	14.151655
17.829683	1090.802864	14.156672
17.832276	1101.122075	14.161690
18.140270	1100.868976	14.166707
18.016976	1092.675516	14.171725
17.738147	1081.382901	14.176743
18.004371	1083.013748	14.181760
17.876434	1093.017771	14.186778
18.074571	1083.934527	14.191795
18.047953	1094.972810	14.196813
18.066083	1095.626720	14.201831
18.065960	1078.801775	14.206848
18.044585	1086.998331	14.211866
18.086234	1090.934017	14.216883
17.845880	1090.566257	14.221901
17.874504	1098.446144	14.226919
18.293382	1096.695247	14.231936
17.954702	1110.853293	14.236954
18.150572	1100.260826	14.241971
17.791675	1101.351586	14.246989
17.993467	1099.488951	14.252007
18.404614	1103.231907	14.257024
18.128822	1104.881474	14.262042
18.147352	1104.929909	14.267059
18.248590	1095.293673	14.272077
17.959147	1104.708159	14.277095
18.205750	1099.225344	14.282112
17.860421	1099.216999	14.287130
17.798537	1092.875280	14.292147
18.073529	1108.651698	14.297165
18.169566	1129.226001	14.302183
18.279163	1128.135755	14.307200
18.365116	1121.404300	14.312218
18.591691	1122.024748	14.317235
18.145735	1128.545525	14.322253
18.445441	1130.643206	14.327271
18.736264	1132.006455	14.332288
18.380749	1124.622484	14.337306
18.510446	1116.842244	14.342323
18.524293	1132.439439	14.347341
18.636810	1132.986822	14.352359
18.611094	1125.912462	14.357376
18.574260	1128.344846	14.362394
18.790365	1123.936567	14.367411
18.702452	1128.004875	14.372429
18.939640	1129.450794	14.377447
18.826285	1120.072606	14.382464
18.671992	1127.425941	14.387482
19.012534	1126.345357	14.392499
18.816193	1124.679593	14.397517
18.954457	1121.305859	14.402535
18.686829	1107.554109	14.407552
18.506738	1127.839454	14.412570
18.581408	1115.872947	14.417587
18.657039	1122.548233	14.422605
18.402380	1124.713908	14.427623
18.717730	1124.001403	14.432640
18.169193	1125.978872	14.437658
18.411059	1115.074120	14.442675
18.692990	1131.982886	14.447693
18.425835	1147.817643	14.452711
19.185941	1140.227257	14.457728
18.967993	1161.888557	14.462746
18.872764	1152.000745	14.467763
19.224922	1155.809162	14.472781
19.045496	1149.407920	14.477799
19.282599	1144.444288	14.482816
19.076526	1148.432932	14.487834
19.328160	1151.439395	14.492851
19.081826	1123.604563	14.497869
18.968852	1122.260794	14.502887
19.067796	1125.033867	14.507904
18.892631	1125.892527	14.512922
19.022621	1145.261639	14.517939
19.227601	1147.343879	14.522957
19.129262	1149.663813	14.527975
19.521827	1154.131385	14.532992
19.114863	1153.245972	14.538010
19.186155	1152.300418	14.543027
19.230235	1148.086675	14.548045
19.278896	1141.877036	14.553063
19.265102	1148.954252	14.558080
18.904144	1157.311081	14.563098
18.877936	1154.012149	14.568115
19.376411	1142.190904	14.573133
19.266824	1155.333342	14.578151
19.626302	1140.874091	14.583168
19.316291	1160.236027	14.588186
19.362325	1151.307583	14.593203
19.270075	1145.359182	14.598221
19.057208	1150.071467	14.603239
19.347521	1149.496737	14.608256
19.583310	1147.802268	14.613274
19.702838	1150.647719	14.618291
19.732301	1152.153947	14.623309
19.524158	1148.112573	14.628327
19.423453	1145.883456	14.633344
19.471836	1138.818101	14.638362
19.484532	1135.107300	14.643379
19.821721	1141.659856	14.648397
19.697400	1138.688900	14.653415
19.732954	1143.405595	14.658432
19.802750	1150.309378	14.663450
19.516981	1144.584068	14.668467
19.908475	1147.487312	14.673485
19.969721	1152.672717	14.678503
19.752756	1140.785089	14.683520
19.587450	1149.832296	14.688538
19.800275	1157.093288	14.693555
19.907659	1145.484284	14.698573
19.965415	1153.564864	14.703591
20.008562	1141.993442	14.708608
20.009543	1154.276605	14.713626
19.553087	1155.169943	14.718643
19.759062	1148.726661	14.723661
19.650010	1151.808082	14.728679
20.082677	1156.283396	14.733696
19.848371	1148.660916	14.738714
19.857228	1171.819533	14.743731
20.120360	1165.379592	14.748749
20.073796	1180.161954	14.753767
20.445532	1165.793553	14.758784
20.197517	1155.497201	14.763802
20.030971	1150.471358	14.768819
19.863042	1153.284405	14.773837
20.466541	1157.144972	14.778855
20.164657	1155.897171	14.783872
19.903104	1151.120258	14.788890
20.049365	1150.463249	14.793907
20.309151	1166.000546	14.798925
20.030485	1177.901469	14.803943
20.614782	1162.210359	14.808960
20.267979	1169.212323	14.813978
20.513069	1172.086429	14.818995
20.374746	1149.659186	14.824013
20.035605	1149.678161	14.829031
20.115630	1167.559547	14.834048
20.398480	1149.107313	14.839066
19.940534	1173.150421	14.844083
20.445964	1162.757303	14.849101
20.560302	1170.118619	14.854119
20.250775	1176.942801	14.859136
20.417483	1158.224757	14.864154
20.317931	1163.657371	14.869171
20.399998	1165.365896	14.874189
20.298210	1165.574546	14.879207
19.970648	1161.765860	14.884224
20.311041	1164.103632	14.889242
20.004878	1158.973321	14.894259
20.834331	1179.179483	14.899277
20.899154	1191.385797	14.904295
20.254871	1177.654110	14.909312
20.498409	1175.384633	14.914330
20.532228	1189.907698	14.919347
21.210371	1181.632920	14.924365
21.002630	1199.469000	14.929383
20.752055	1182.045277	14.934400
20.833953	1166.465530	14.939418
20.574138	1171.653220	14.944435
21.126364	1166.439310	14.949453
20.471770	1163.702807	14.954471
20.770755	1177.106233	14.959488
20.789928	1189.737344	14.964506
20.704500	1191.474733	14.969523
21.104436	1196.423699	14.974541
21.172272	1200.236600	14.979559
20.964634	1177.246850	14.984576
21.060671	1186.657909	14.989594
21.128542	1196.638498	14.994611
21.065467	1174.235392	14.999629
21.277913	1173.779221	15.004647
21.059213	1170.580589	15.009664
20.658449	1157.264114	15.014682
20.698704	1183.090543	15.019699
20.999395	1191.995028	15.024717
20.242433	1188.378734	15.029735
20.690477	1192.527161	15.034752
20.857219	1193.854040	15.039770
20.816321	1199.891637	15.044787
21.214973	1210.136219	15.049805
21.336237	1213.064058	15.054823
21.325365	1214.597822	15.059840
21.743923	1218.766678	15.064858
21.152791	1209.826782	15.069875
21.504271	1194.891518	15.074893
21.352708	1194.278608	15.079911
21.300746	1204.959012	15.084928
21.321694	1197.994604	15.089946
21.377816	1202.649659	15.094963
21.248828	1193.668828	15.099981
21.323827	1204.333368	15.104999
21.912459	1217.169559	15.110016
21.746379	1203.622166	15.115034
21.153785	1195.462118	15.120051
21.621242	1197.471663	15.125069
21.543604	1206.064919	15.130087
21.541114	1199.205156	15.135104
21.602742	1203.334387	15.140122
21.478882	1202.373253	15.145139
21.366890	1208.790849	15.150157
21.498058	1218.722415	15.155175
21.733172	1221.404313	15.160192
21.848222	1218.755734	15.165210
21.818417	1215.322760	15.170227
22.081840	1225.193503	15.175245
21.644968	1213.790317	15.180263
21.651616	1210.310775	15.185280
21.871523	1209.238115	15.190298
21.893645	1213.254999	15.195315
22.148677	1220.528531	15.200333
21.747097	1199.672624	15.205351
21.393859	1203.025080	15.210368
22.058902	1203.279615	15.215386
22.017441	1214.954586	15.220403
22.073172	1222.436224	15.225421
22.085101	1214.783647	15.230439
21.983011	1201.889942	15.235456
22.349466	1193.774523	15.240474
21.807956	1185.885717	15.245491
21.483522	1188.178857	15.250509
21.986343	1198.173578	15.255527
21.912477	1203.762368	15.260544
22.339521	1211.025577	15.265562
22.520235	1217.501678	15.270579
22.157821	1209.075668	15.275597
22.116037	1211.990695	15.280615
22.105781	1212.111592	15.285632
22.207871	1213.788276	15.290650
22.133603	1208.981575	15.295667
21.986147	1199.272415	15.300685
22.210197	1210.425433	15.305703
21.924401	1210.476923	15.310720
22.252132	1204.891111	15.315738
22.192297	1219.047656	15.320755
22.328131	1208.831906	15.325773
22.164268	1200.217799	15.330791
22.148920	1215.391822	15.335808
22.420734	1204.096294	15.340826
21.728098	1223.106057	15.345843
22.179191	1240.183806	15.350861
22.196172	1234.924489	15.355879
21.904420	1240.650464	15.360896
22.442553	1237.017347	15.365914
22.261859	1237.955852	15.370931
22.429813	1246.858883	15.375949
22.388732	1242.009488	15.380967
22.260215	1244.913268	15.385984
22.450650	1257.714920	15.391002
22.868106	1269.777799	15.396019
23.271522	1259.095028	15.401037
23.638436	1246.460735	15.406055
23.269682	1241.894391	15.411072
22.961343	1230.641773	15.416090
22.833558	1224.940120	15.421107
22.794270	1238.428040	15.426125
23.072891	1236.757974	15.431143
22.867421	1229.139348	15.436160
22.966941	1228.170427	15.441178
22.977277	1235.212991	15.446195
22.841191	1238.260714	15.451213
23.174148	1230.341331	15.456231
22.959702	1237.599361	15.461248
22.811989	1233.543254	15.466266
22.918295	1231.383835	15.471283
22.852357	1223.046596	15.476301
23.162068	1226.903377	15.481319
22.988571	1238.785786	15.486336
23.274950	1225.042951	15.491354
23.317026	1237.742747	15.496371
23.745989	1238.116402	15.501389
23.814473	1223.724648	15.506407
23.264735	1219.363192	15.511424
23.210607	1200.786101	15.516442
22.973057	1197.594515	15.521459
22.755361	1202.280847	15.526477
23.205645	1218.035691	15.531495
23.227887	1227.454050	15.536512
23.261441	1233.448260	15.541530
23.248418	1226.758111	15.546547
22.996243	1226.264762	15.551565
23.401673	1228.480396	15.556583
23.238593	1227.290347	15.561600
23.336564	1221.651764	15.566618
23.192256	1228.704726	15.571635
23.172800	1226.656234	15.576653
23.314473	1219.079048	15.581671
23.195528	1226.938120	15.586688
23.427206	1223.026176	15.591706
23.345640	1239.165146	15.596723
23.437353	1249.388443	15.601741
23.965485	1250.707171	15.606759
23.578878	1256.284287	15.611776
23.742459	1259.693647	15.616794
23.804923	1253.306513	15.621811
23.619454	1264.346566	15.626829
23.699186	1251.732960	15.631847
23.605580	1257.723590	15.636864
23.790409	1259.721986	15.641882
23.961592	1252.411320	15.646899
23.825584	1260.922339	15.651917
23.813587	1249.327475	15.656935
23.645124	1257.569686	15.661952
24.138931	1254.435544	15.666970
24.052720	1263.416999	15.671987
24.086421	1254.675149	15.677005
24.155521	1253.544744	15.682023
23.724308	1263.863324	15.687040
24.139132	1251.528738	15.692058
24.209174	1254.553422	15.697075
23.760018	1261.276522	15.702093
24.016584	1248.685262	15.707111
23.817141	1251.232122	15.712128
24.211017	1251.657238	15.717146
24.199039	1251.996299	15.722163
23.824440	1261.228528	15.727181
24.094139	1246.762365	15.732199
23.922078	1255.350390	15.737216
23.936558	1246.383805	15.742234
23.781480	1253.484417	15.747251
23.785887	1263.767616	15.752269
24.318345	1260.130511	15.757287
24.172597	1285.471200	15.762304
24.350082	1282.488524	15.767322
24.718155	1286.603154	15.772339
24.217367	1283.830189	15.777357
24.712175	1281.257009	15.782375
24.740438	1293.035853	15.787392
24.969429	1286.818792	15.792410
24.776412	1258.734193	15.797427
24.581284	1246.767099	15.802445
24.288795	1247.862443	15.807463
24.425385	1250.539568	15.812480
24.577398	1246.116850	15.817498
24.646712	1254.552406	15.822515
24.598774	1269.022138	15.827533
24.543380	1271.025790	15.832551
24.330743	1286.066174	15.837568
24.718449	1281.008528	15.842586
24.815763	1278.758279	15.847603
24.717076	1288.619428	15.852621
24.863279	1277.849053	15.857639
24.845125	1285.790105	15.862656
24.889309	1282.218531	15.867674
24.712202	1277.398690	15.872691
24.743845	1291.073919	15.877709
24.721763	1282.318244	15.882727
24.725333	1279.994131	15.887744
24.537637	1280.850541	15.892762
24.728354	1280.308995	15.897779
24.216285	1279.636188	15.902797
24.780730	1283.837637	15.907815
25.132239	1301.726078	15.912832
25.359881	1296.277424	15.917850
25.662958	1299.027422	15.922867
25.503329	1282.398862	15.927885
25.541946	1265.730277	15.932903
25.397473	1270.477548	15.937920
25.346918	1259.725136	15.942938
25.435748	1258.368278	15.947955
25.126905	1277.699464	15.952973
25.390396	1265.943528	15.957991
25.449008	1263.957511	15.963008
25.249039	1263.950337	15.968026
25.413492	1271.942098	15.973043
25.159069	1269.428376	15.978061
25.226928	1270.498417	15.983079
25.388266	1262.634737	15.988096
25.145812	1263.837543	15.993114
25.438575	1263.712727	15.998131
25.168938	1268.141169	16.003149
25.537303	1274.048377	16.008167
25.744546	1262.186796	16.013184
25.116381	1266.590641	16.018202
25.406729	1280.333130	16.023219
25.609376	1289.310165	16.028237
25.862885	1290.765014	16.033255
25.755410	1294.640763	16.038272
25.485149	1296.505151	16.043290
25.856509	1292.453785	16.048307
25.341347	1297.258977	16.053325
25.714186	1287.616314	16.058343
25.695502	1297.637449	16.063360
25.592728	1287.691160	16.068378
25.695519	1286.393990	16.073395
25.815517	1295.870831	16.078413
25.824099	1287.228177	16.083431
25.827035	1302.930088	16.088448
25.702637	1302.620116	16.093466
25.785061	1286.087160	16.098483
25.661382	1298.564831	16.103501
25.912164	1297.453604	16.108519
25.769642	1311.843746	16.113536
26.306361	1330.627848	16.118554
26.588896	1308.520921	16.123571
25.837583	1305.879497	16.128589
26.214663	1303.050024	16.133607
26.169554	1301.909163	16.138624
26.034702	1310.581214	16.143642
26.401014	1318.006259	16.148659
26.245067	1314.618317	16.153677
26.326644	1305.590223	16.158695
26.389823	1310.081571	16.163712
26.223257	1307.311629	16.168730
26.528009	1300.508903	16.173747
26.515069	1317.775807	16.178765
26.477944	1301.668040	16.183783
26.879230	1301.879762	16.188800
26.223816	1293.973705	16.193818
26.374550	1279.369322	16.198835
26.313735	1297.719733	16.203853
26.334921	1322.135398	16.208871
26.244946	1313.371834	16.213888
26.619274	1315.990197	16.218906
26.940684	1316.167883	16.223923
26.658517	1313.260374	16.228941
26.294509	1313.455872	16.233959
26.825780	1314.817191	16.238976
26.517396	1319.574245	16.243994
26.785507	1313.739624	16.249011
26.563613	1317.282570	16.254029
26.801726	1319.738238	16.259047
26.800603	1316.868129	16.264064
26.460265	1323.944280	16.269082
26.792943	1310.876683	16.274099
26.415589	1317.416315	16.279117
26.514212	1330.570550	16.284135
26.696297	1323.971129	16.289152
26.799878	1344.765503	16.294170
27.251203	1336.789307	16.299187
27.103193	1336.206704	16.304205
27.120161	1345.163282	16.309223
27.199921	1353.402314	16.314240
27.119216	1342.874478	16.319258
27.144893	1345.493976	16.324275
27.323064	1339.243369	16.329293
27.034801	1338.393634	16.334311
27.391459	1341.469380	16.339328
27.089617	1338.066770	16.344346
27.242785	1328.069695	16.349363
27.191764	1346.732671	16.354381
26.954784	1339.159152	16.359399
27.471874	1343.828216	16.364416
27.284172	1343.732414	16.369434
27.418102	1336.088153	16.374451
27.560265	1332.239983	16.379469
27.463350	1336.701308	16.384487
27.487202	1332.834506	16.389504
27.202216	1339.300821	16.394522
27.645721	1343.654930	16.399539
27.668137	1340.048559	16.404557
27.149220	1330.759505	16.409575
27.421832	1328.474179	16.414592
27.284708	1344.414403	16.419610
27.819904	1336.484179	16.424627
27.764716	1336.578256	16.429645
27.504749	1353.305010	16.434663
27.605008	1333.197554	16.439680
27.545976	1356.023627	16.444698
27.558255	1362.195785	16.449715
27.567788	1368.061754	16.454733
27.730870	1381.005213	16.459751
27.651845	1371.917413	16.464768
27.935203	1365.155000	16.469786
28.107012	1373.491019	16.474803
28.135165	1374.909310	16.479821
28.085433	1361.314405	16.484839
28.705882	1360.430819	16.489856
28.340229	1363.271069	16.494874
28.247653	1363.390416	16.499891
28.370354	1352.186537	16.504909
28.268449	1331.510813	16.509927
28.408962	1330.800424	16.514944
27.943474	1334.499557	16.519962
28.102622	1324.535153	16.524979
28.398850	1329.056684	16.529997
28.355261	1327.048775	16.535015
28.579991	1319.000405	16.540032
28.218168	1324.332936	16.545050
27.994099	1319.684006	16.550067
28.272123	1331.690658	16.555085
28.330197	1351.735002	16.560103
28.697613	1355.741311	16.565120
28.446677	1347.457604	16.570138
28.389748	1340.939203	16.575155
28.364235	1355.564932	16.580173
28.412148	1349.055773	16.585191
28.895971	1351.819015	16.590208
28.462168	1349.775013	16.595226
28.437808	1358.826014	16.600243
28.985708	1351.909080	16.605261
28.908695	1357.317765	16.610279
28.869653	1344.432810	16.615296
28.639924	1334.002627	16.620314
28.337073	1340.898011	16.625331
28.530951	1344.985153	16.630349
28.531376	1353.486469	16.635367
28.959731	1355.119486	16.640384
28.819245	1358.126824	16.645402
28.623134	1357.052638	16.650419
28.957173	1358.995882	16.655437
28.552603	1365.614430	16.660455
28.670545	1360.185259	16.665472
28.597210	1360.340791	16.670490
28.596319	1368.443576	16.675507
29.085973	1373.856244	16.680525
29.066696	1389.240506	16.685543
29.144540	1383.478634	16.690560
29.171732	1379.814978	16.695578
29.175161	1384.881885	16.700595
29.221707	1378.848261	16.705613
29.227211	1378.059803	16.710631
29.417608	1381.041200	16.715648
29.219140	1388.641097	16.720666
29.338357	1377.771977	16.725683
29.532276	1379.883042	16.730701
29.448567	1381.401107	16.735719
29.461946	1366.766001	16.740736
29.584026	1373.091646	16.745754
29.308910	1369.863128	16.750771
29.588266	1372.039391	16.755789
29.676024	1382.038661	16.760807
29.519590	1365.665940	16.765824
29.393010	1387.479558	16.770842
29.500120	1383.311036	16.775859
29.732064	1377.415056	16.780877
29.567932	1383.551228	16.785895
29.802207	1377.631244	16.790912
29.578666	1378.719335	16.795930
29.411660	1384.586142	16.800947
29.584391	1379.244353	16.805965
29.663196	1379.682964	16.810983
29.805921	1390.775745	16.816000
30.010310	1403.500815	16.821018
30.105351	1409.804373	16.826035
30.125001	1379.287522	16.831053
30.177642	1375.823567	16.836071
29.878712	1377.891096	16.841088
29.834029	1379.931175	16.846106
29.815491	1383.190568	16.851123
30.066402	1392.738931	16.856141
30.032939	1404.894148	16.861159
30.186486	1403.100662	16.866176
29.796783	1405.211735	16.871194
30.262691	1403.861830	16.876211
30.176490	1400.063584	16.881229
30.051353	1411.715726	16.886247
30.108723	1407.307225	16.891264
30.393390	1408.137345	16.896282
29.929239	1412.353914	16.901299
30.130929	1402.533391	16.906317
30.121671	1413.582614	16.911335
30.491325	1406.547693	16.916352
30.221779	1407.637681	16.921370
30.140278	1432.923711	16.926387
30.470426	1428.007202	16.931405
30.559532	1430.064149	16.936423
30.605899	1431.481404	16.941440
30.943525	1423.049810	16.946458
30.729568	1424.607314	16.951475
30.981023	1429.984181	16.956493
30.825613	1427.529058	16.961511
30.694257	1411.597747	16.966528
31.264079	1406.887468	16.971546
30.549121	1393.152897	16.976563
30.532534	1392.180518	16.981581
30.744882	1409.595897	16.986599
31.153176	1419.940391	16.991616
31.500374	1415.989428	16.996634
31.062383	1403.533881	17.001651
30.980367	1393.553192	17.006669
30.997571	1399.121493	17.011687
30.813180	1396.235993	17.016704
30.895772	1396.519278	17.021722
30.921465	1410.759095	17.026739
31.164773	1420.663207	17.031757
31.505932	1417.728052	17.036775
31.416838	1415.121049	17.041792
31.132542	1407.453164	17.046810
30.866959	1420.400774	17.051827
31.201641	1424.566032	17.056845
31.374100	1418.682031	17.061863
31.441812	1412.640763	17.066880
31.520181	1417.726985	17.071898
31.576154	1425.166365	17.076915
31.551509	1411.998701	17.081933
31.494950	1419.431285	17.086951
31.773958	1413.687332	17.091968
31.781173	1425.299112	17.096986
31.554082	1426.657636	17.102003
31.389009	1420.340706	17.107021
31.362443	1408.967584	17.112039
31.351144	1411.307814	17.117056
31.580458	1417.533879	17.122074
31.526155	1430.800073	17.127091
31.405343	1416.916318	17.132109
31.374686	1416.525902	17.137127
31.490338	1419.832801	17.142144
31.504663	1429.923163	17.147162
31.642450	1446.905499	17.152179
31.664658	1451.431412	17.157197
31.824525	1448.995434	17.162215
31.771080	1458.887792	17.167232
31.957739	1451.587466	17.172250
32.024006	1446.300053	17.177267
31.935937	1457.612689	17.182285
31.999372	1454.862772	17.187303
31.763921	1454.372556	17.192320
32.363309	1448.733891	17.197338
31.985126	1454.915699	17.202355
31.912288	1443.151044	17.207373
32.276162	1461.307471	17.212391
32.428638	1459.544072	17.217408
32.614780	1455.419351	17.222426
32.246924	1451.536553	17.227443
32.100733	1450.744227	17.232461
32.195419	1445.464124	17.237479
32.658579	1463.920242	17.242496
32.511990	1463.570633	17.247514
32.361362	1472.530773	17.252531
32.343000	1466.112229	17.257549
32.618910	1463.309484	17.262567
32.647851	1462.898393	17.267584
32.603209	1459.771511	17.272602
32.556659	1460.810677	17.277619
32.749341	1468.631365	17.282637
32.830957	1464.491636	17.287655
32.863807	1457.998303	17.292672
32.943492	1452.319948	17.297690
33.098600	1461.722792	17.302707
32.670934	1461.369837	17.307725
32.761750	1459.242272	17.312743
32.648172	1457.684234	17.317760
32.764527	1459.767976	17.322778
32.447615	1458.768857	17.327795
32.939002	1451.682897	17.332813
33.168711	1453.166692	17.337831
32.595795	1455.326944	17.342848
33.182543	1444.280136	17.347866
32.913795	1460.422322	17.352883
33.029963	1463.746664	17.357901
33.190952	1482.262186	17.362919
33.460101	1483.325156	17.367936
33.752929	1469.724915	17.372954
33.589136	1464.656394	17.377971
33.518955	1464.017427	17.382989
33.649213	1444.079056	17.388007
33.223631	1446.629267	17.393024
33.339063	1445.485878	17.398042
33.356720	1451.167098	17.403059
33.059067	1441.241301	17.408077
33.145943	1460.715167	17.413095
33.740796	1474.555519	17.418112
33.934252	1478.812034	17.423130
33.729581	1479.692319	17.428147
33.989520	1483.705401	17.433165
33.842984	1471.947786	17.438183
33.125811	1471.123850	17.443200
33.545744	1478.038610	17.448218
33.642473	1478.597079	17.453235
33.581722	1478.663144	17.458253
33.732079	1486.331409	17.463271
33.544879	1470.950329	17.468288
33.756448	1479.982686	17.473306
33.722648	1484.991221	17.478323
33.656660	1480.392288	17.483341
34.405992	1490.979838	17.488359
33.890590	1506.957548	17.493376
34.172721	1510.523136	17.498394
34.157538	1510.134686	17.503411
34.088839	1515.863070	17.508429
34.365703	1501.568885	17.513447
34.310182	1510.777662	17.518464
34.743333	1504.847006	17.523482
34.731487	1491.905669	17.528499
34.446588	1485.781521	17.533517
34.483642	1467.175852	17.538535
34.491306	1466.623416	17.543552
34.679443	1467.455713	17.548570
34.376754	1469.463845	17.553587
34.296947	1471.126922	17.558605
34.573824	1479.464530	17.563623
34.099421	1476.229164	17.568640
34.592380	1482.560681	17.573658
34.918974	1502.659260	17.578675
34.370721	1491.208335	17.583693
35.022731	1486.083720	17.588711
34.625357	1485.605893	17.593728
35.012556	1481.350513	17.598746
34.727203	1478.306510	17.603763
34.618792	1474.658745	17.608781
34.675190	1487.995265	17.613799
34.642026	1497.783130	17.618816
34.922047	1493.541128	17.623834
35.097003	1498.236272	17.628851
34.692997	1492.971448	17.633869
34.704694	1501.621356	17.638887
34.865730	1498.375844	17.643904
34.987967	1496.334013	17.648922
34.721366	1495.501749	17.653939
34.975308	1501.745232	17.658957
34.890360	1519.810371	17.663975
34.949425	1532.137183	17.668992
35.321840	1530.025859	17.674010
35.523305	1530.602844	17.679027
35.355520	1534.611240	17.684045
35.802584	1520.363310	17.689063
35.473948	1529.941793	17.694080
35.471462	1519.406223	17.699098
35.489025	1524.591296	17.704115
35.819259	1529.767214	17.709133
35.797845	1526.058413	17.714151
35.843063	1528.421206	17.719168
35.529582	1518.066540	17.724186
35.822986	1512.370952	17.729203
35.640062	1518.899598	17.734221
35.614392	1519.087210	17.739239
35.463552	1524.536496	17.744256
35.808218	1521.403330	17.749274
35.848860	1525.117278	17.754291
36.132291	1524.484626	17.759309
35.974023	1520.292214	17.764327
35.738307	1522.110177	17.769344
35.841765	1525.234692	17.774362
35.959709	1519.650566	17.779379
35.723016	1519.919106	17.784397
35.801416	1518.422040	17.789415
35.670010	1513.086967	17.794432
35.862965	1526.879429	17.799450
36.046595	1529.118378	17.804467
35.956408	1536.458755	17.809485
36.167313	1542.194282	17.814503
36.065014	1539.973243	17.819520
36.287938	1535.633790	17.824538
36.419216	1534.251589	17.829555
36.281116	1539.536396	17.834573
36.354561	1543.314799	17.839591
36.348685	1541.265201	17.844608
36.345948	1533.344651	17.849626
36.281884	1544.490218	17.854643
36.428277	1565.824985	17.859661
36.749667	1564.466277	17.864679
36.569970	1565.784505	17.869696
36.467415	1565.385299	17.874714
36.579474	1560.424092	17.879731
36.924474	1572.579488	17.884749
36.848803	1574.833346	17.889767
36.598801	1571.177465	17.894784
36.392367	1562.602074	17.899802
36.851345	1570.345938	17.904819
36.595261	1561.230207	17.909837
37.122933	1560.437721	17.914855
36.559455	1562.313198	17.919872
37.029544	1573.639769	17.924890
37.250835	1574.326849	17.929907
37.019367	1578.479423	17.934925
37.272070	1575.757058	17.939943
37.412303	1596.538238	17.944960
37.411366	1583.656037	17.949978
37.645517	1569.645777	17.954995
37.497806	1575.934015	17.960013
37.511565	1552.269801	17.965031
37.244904	1560.614217	17.970048
37.441892	1557.769781	17.975066
37.588202	1562.165981	17.980083
37.480809	1566.862537	17.985101
37.460779	1559.781133	17.990119
37.477030	1557.383633	17.995136
37.644009	1558.376890	18.000154
37.657185	1560.000008	18.005171
37.293717	1567.635526	18.010189
37.497241	1582.803660	18.015207
37.578196	1586.209624	18.020224
37.742170	1597.019554	18.025242
37.940484	1584.192208	18.030259
37.692910	1595.995610	18.035277
37.911316	1593.719991	18.040295
37.880215	1590.970715	18.045312
37.559349	1584.621991	18.050330
37.983314	1587.197362	18.055347
37.910147	1597.142077	18.060365
37.807003	1580.247792	18.065383
37.887051	1596.033703	18.070400
37.798585	1610.973383	18.075418
38.106742	1614.674439	18.080435
38.393824	1614.099244	18.085453
38.391517	1616.052835	18.090471
38.412674	1602.872321	18.095488
38.805921	1617.381663	18.100506
38.628306	1613.149122	18.105523
38.446645	1619.672484	18.110541
38.593060	1609.394885	18.115559
38.703314	1618.656046	18.120576
38.134796	1616.515977	18.125594
38.971982	1610.783043	18.130611
38.360333	1626.936997	18.135629
38.745731	1614.099179	18.140647
38.826433	1613.263248	18.145664
38.884181	1609.083926	18.150682
38.939605	1605.395868	18.155699
38.889421	1616.087483	18.160717
38.686929	1613.817055	18.165735
38.830471	1620.811999	18.170752
38.739272	1613.573259	18.175770
38.942321	1609.365005	18.180787
38.631641	1613.420261	18.185805
38.931539	1609.379049	18.190823
38.981864	1617.404022	18.195840
39.061832	1608.748997	18.200858
38.918804	1600.920681	18.205875
38.674315	1619.055208	18.210893
38.744479	1620.948208	18.215911
39.057432	1632.696996	18.220928
39.158288	1639.927909	18.225946
39.173439	1633.135106	18.230963
39.205215	1645.018743	18.235981
39.305416	1640.799725	18.240999
39.317358	1633.765948	18.246016
39.298108	1637.943106	18.251034
39.383900	1639.764243	18.256051
39.410602	1648.171038	18.261069
39.690514	1660.855106	18.266087
40.145663	1658.939120	18.271104
40.224167	1647.399069	18.276122
40.281527	1637.427272	18.281139
40.012774	1629.795088	18.286157
39.946551	1623.313530	18.291175
39.975021	1623.300096	18.296192
39.635093	1628.599982	18.301210
40.138447	1625.585828	18.306227
39.895069	1632.623264	18.311245
39.857748	1628.289985	18.316263
40.038138	1618.059319	18.321280
39.525972	1633.734303	18.326298
39.706448	1622.096919	18.331315
39.909058	1641.684548	18.336333
39.929538	1650.425989	18.341351
40.043722	1653.891232	18.346368
40.075144	1663.760446	18.351386
40.324899	1652.591448	18.356403
40.279236	1662.653298	18.361421
40.195604	1659.101774	18.366439
40.538447	1657.310240	18.371456
40.193909	1659.544377	18.376474
40.588112	1661.125205	18.381491
40.502283	1648.459510	18.386509
40.573820	1656.407977	18.391527
40.743983	1652.900920	18.396544
40.639927	1654.931951	18.401562
40.890305	1652.869121	18.406579
40.998112	1657.385673	18.411597
40.688786	1651.885885	18.416615
40.641373	1651.041402	18.421632
41.006161	1670.872901	18.426650
41.277735	1677.531203	18.431667
41.166436	1680.166899	18.436685
40.915353	1656.287271	18.441703
41.116984	1656.144644	18.446720
40.966005	1658.767014	18.451738
41.332024	1673.703491	18.456755
41.513732	1672.644199	18.461773
41.108125	1659.893168	18.466791
41.574056	1656.003026	18.471808
41.012428	1648.355066	18.476826
41.363833	1663.900167	18.481843
41.234453	1670.483209	18.486861
41.084748	1670.058136	18.491879
41.635386	1678.036874	18.496896
41.370184	1677.461224	18.501914
41.482269	1663.852300	18.506931
41.697446	1671.899265	18.511949
41.275739	1670.938509	18.516967
41.657665	1673.261034	18.521984
41.266775	1676.812503	18.527002
41.302774	1670.494718	18.532019
41.444476	1678.367633	18.537037
41.717615	1695.417629	18.542055
41.755122	1707.232463	18.547072
41.974724	1709.690859	18.552090
42.308246	1701.290497	18.557107
42.137566	1704.251717	18.562125
42.205138	1698.588066	18.567143
42.431266	1699.296004	18.572160
42.000328	1707.215342	18.577178
42.050814	1700.801659	18.582195
42.594410	1692.495900	18.587213
42.541299	1694.061885	18.592231
42.407189	1668.730220	18.597248
41.968612	1674.983505	18.602266
42.223143	1674.288900	18.607283
42.414894	1683.855095	18.612301
42.467122	1698.569274	18.617319
42.741112	1694.392969	18.622336
42.515672	1689.717778	18.627354
42.542808	1700.338808	18.632371
42.651245	1690.822057	18.637389
42.296058	1693.073705	18.642407
42.704360	1697.068428	18.647424
42.677163	1693.665620	18.652442
42.598841	1699.134476	18.657459
42.632989	1694.983634	18.662477
42.414277	1704.201978	18.667495
43.022321	1694.914236	18.672512
42.708804	1697.196001	18.677530
42.732740	1695.119806	18.682547
43.115009	1705.220598	18.687565
42.914244	1706.227989	18.692583
43.057689	1703.007779	18.697600
43.370396	1718.013338	18.702618
42.854208	1719.190162	18.707635
43.163176	1722.155379	18.712653
43.161008	1725.971122	18.717671
43.407988	1721.248164	18.722688
43.145479	1722.331302	18.727706
42.938274	1721.291793	18.732723
43.657959	1718.320405	18.737741
43.168022	1717.367968	18.742759
43.436118	1710.158576	18.747776
43.080409	1718.304040	18.752794
43.449577	1729.751721	18.757811
43.584062	1725.592951	18.762829
43.471720	1741.292118	18.767847
43.682096	1743.058038	18.772864
43.839661	1746.201213	18.777882
43.632059	1756.290869	18.782899
43.819077	1745.753352	18.787917
43.575266	1750.408539	18.792935
43.930547	1751.634241	18.797952
43.887105	1746.525268	18.802970
43.426732	1757.405617	18.807987
43.965305	1769.955702	18.813005
44.105419	1765.085254	18.818023
44.497879	1775.701666	18.823040
44.161798	1770.533971	18.828058
44.335017	1767.345634	18.833075
44.908623	1774.196753	18.838093
44.421156	1771.729134	18.843111
44.565159	1770.536517	18.848128
44.466173	1769.348822	18.853146
44.393046	1771.252333	18.858163
44.463482	1764.121440	18.863181
44.298644	1773.221683	18.868199
44.302610	1758.333265	18.873216
44.805397	1767.207248	18.878234
44.556992	1771.323307	18.883251
44.444790	1761.286942	18.888269
44.318821	1776.577031	18.893287
44.641009	1787.270410	18.898304
44.804415	1786.189532	18.903322
44.712410	1796.438435	18.908339
45.605618	1799.667311	18.913357
44.954765	1798.139567	18.918375
45.132971	1799.042414	18.923392
45.244012	1798.343567	18.928410
45.269132	1803.564292	18.933427
45.633223	1799.583083	18.938445
45.655472	1794.002271	18.943463
45.421462	1787.152752	18.948480
45.191677	1773.902748	18.953498
44.873899	1772.264656	18.958515
45.666730	1789.282019	18.963533
45.771845	1804.580400	18.968551
45.884934	1795.674748	18.973568
45.868833	1779.448060	18.978586
45.314564	1764.774507	18.983603
45.668480	1764.884632	18.988621
45.544065	1773.511719	18.993639
45.945008	1777.661794	18.998656
45.823286	1790.183432	19.003674
45.715236	1790.604317	19.008691
45.589726	1785.895656	19.013709
45.704975	1797.007050	19.018727
45.549620	1786.473531	19.023744
45.713914	1790.270246	19.028762
45.934194	1786.923950	19.033779
46.136632	1783.335358	19.038797
46.085340	1793.787545	19.043815
46.046186	1780.425334	19.048832
46.045411	1779.579632	19.053850
46.096787	1802.764453	19.058867
46.606748	1806.997099	19.063885
46.690025	1806.414047	19.068903
46.321731	1813.356867	19.073920
46.515597	1804.253239	19.078938
46.610115	1807.374566	19.083955
46.890772	1807.462156	19.088973
46.587164	1817.210674	19.093991
46.574455	1817.219398	19.099008
46.784230	1803.790639	19.104026
46.481286	1824.497154	19.109043
46.854723	1808.433200	19.114061
46.838697	1811.713132	19.119079
46.576816	1811.517589	19.124096
46.571742	1794.852501	19.129114
46.408910	1806.174598	19.134131
46.783148	1812.824065	19.139149
46.890613	1824.882515	19.144167
46.905987	1834.343321	19.149184
47.035726	1833.550252	19.154202
47.451132	1835.731459	19.159219
47.326727	1827.431897	19.164237
47.539548	1829.170458	19.169255
47.413562	1833.635550	19.174272
47.810173	1827.286255	19.179290
47.393995	1829.890085	19.184307
47.780540	1832.572064	19.189325
47.632164	1830.922505	19.194343
48.105637	1830.627094	19.199360
47.649241	1815.364554	19.204378
47.423899	1822.017055	19.209395
47.748132	1821.963996	19.214413
47.744832	1828.453642	19.219431
47.697860	1832.360664	19.224448
47.813889	1824.266419	19.229466
47.697970	1823.526740	19.234483
47.859046	1826.141069	19.239501
47.656481	1825.720790	19.244519
47.853887	1818.273060	19.249536
47.946680	1826.082291	19.254554
47.807231	1830.528153	19.259571
48.076587	1840.244002	19.264589
48.004623	1857.451196	19.269607
48.062737	1862.453128	19.274624
48.272476	1850.357050	19.279642
48.154955	1859.065122	19.284659
48.581832	1850.249694	19.289677
48.250554	1844.492471	19.294695
48.050008	1858.718128	19.299712
48.274041	1846.021338	19.304730
48.399376	1857.644826	19.309747
48.864633	1880.330121	19.314765
48.824567	1880.950380	19.319783
48.928667	1880.882524	19.324800
48.950301	1885.325007	19.329818
48.987833	1883.546504	19.334835
49.438995	1873.511248	19.339853
48.861460	1856.267546	19.344871
48.805503	1842.521293	19.349888
49.207793	1853.414054	19.354906
49.249255	1862.909735	19.359923
49.170611	1848.124831	19.364941
49.404887	1850.377700	19.369959
48.798498	1854.519479	19.374976
49.204876	1869.428220	19.379994
48.864321	1880.276258	19.385011
48.952180	1874.347017	19.390029
49.253528	1881.057174	19.395047
49.181648	1879.950612	19.400064
49.672203	1871.167951	19.405082
49.457804	1870.009753	19.410099
49.408505	1874.092149	19.415117
49.563304	1878.881479	19.420135
49.719024	1889.453441	19.425152
49.944713	1885.257511	19.430170
49.794585	1892.959693	19.435187
49.944011	1899.669180	19.440205
49.926492	1886.067109	19.445223
49.795170	1893.350485	19.450240
49.773486	1890.366358	19.455258
49.837080	1900.145969	19.460275
50.313237	1885.902933	19.465293
50.249480	1882.858052	19.470311
50.071686	1887.334280	19.475328
50.238982	1884.355338	19.480346
50.322148	1885.218784	19.485363
50.386441	1884.527462	19.490381
50.419248	1892.938697	19.495399
50.419350	1911.024094	19.500416
50.800594	1908.507766	19.505434
50.642074	1906.908491	19.510451
50.611611	1917.066212	19.515469
50.313103	1907.752978	19.520487
50.367517	1913.257055	19.525504
50.806169	1912.610548	19.530522
50.850362	1909.672808	19.535539
50.676288	1918.242836	19.540557
50.758126	1911.068263	19.545575
50.833664	1918.064740	19.550592
50.905863	1912.095951	19.555610
51.220027	1914.068730	19.560627
51.093970	1931.080638	19.565645
51.482986	1933.858672	19.570663
51.392696	1920.128062	19.575680
51.511095	1912.593748	19.580698
51.316410	1904.532896	19.585715
50.995622	1910.151921	19.590733
51.566379	1924.544042	19.595751
51.703239	1919.188902	19.600768
51.909980	1928.870672	19.605786
52.100090	1931.687875	19.610803
51.940919	1913.207194	19.615821
52.009048	1907.184361	19.620839
51.913199	1903.947361	19.625856
51.582665	1896.893690	19.630874
51.693298	1903.040365	19.635891
51.674262	1895.086303	19.640909
51.470364	1898.432925	19.645927
51.563616	1915.440854	19.650944
52.107073	1926.055448	19.655962
51.975665	1923.576005	19.660979
52.303305	1930.816424	19.665997
51.944681	1926.122032	19.671015
52.041207	1922.377702	19.676032
52.201487	1926.841966	19.681050
52.262223	1924.522087	19.686067
52.226655	1924.388739	19.691085
52.367268	1920.207055	19.696103
52.272304	1923.287679	19.701120
52.470374	1937.493791	19.706138
52.542703	1952.067308	19.711155
52.625016	1946.885328	19.716173
52.965542	1940.347837	19.721191
52.888311	1957.715049	19.726208
52.795183	1953.228715	19.731226
52.980235	1956.850014	19.736243
52.980310	1952.004813	19.741261
53.149208	1948.357560	19.746279
52.980724	1952.601782	19.751296
52.975525	1948.408561	19.756314
53.055701	1949.496102	19.761331
52.568048	1956.208345	19.766349
53.150078	1949.222326	19.771367
53.013533	1958.513256	19.776384
53.233460	1957.310637	19.781402
53.246794	1966.672857	19.786419
53.589847	1983.108145	19.791437
53.917953	1977.204707	19.796455
53.561497	1981.662066	19.801472
53.776872	1982.095054	19.806490
53.929650	1976.073362	19.811507
53.667501	1975.151564	19.816525
54.005423	1973.359234	19.821543
53.586437	1974.451122	19.826560
53.701052	1958.934451	19.831578
53.754973	1974.917172	19.836595
53.802641	1975.648710	19.841613
53.998044	1965.823947	19.846631
54.088670	1972.296361	19.851648
54.068152	1954.144056	19.856666
54.152020	1960.647499	19.861683
53.886310	1971.022654	19.866701
54.140071	1966.415219	19.871719
53.927710	2000.128569	19.876736
54.071493	1998.324031	19.881754
54.085817	2004.750609	19.886771
54.149211	2004.148200	19.891789
54.511909	2002.784598	19.896807
54.290075	2015.913644	19.901824
54.430097	2013.268086	19.906842
54.577022	2017.073436	19.911859
54.736443	2024.438537	19.916877
55.171549	2014.665461	19.921895
55.154139	2025.144880	19.926912
55.232484	2024.064461	19.931930
55.649522	2016.146136	19.936947
55.387149	2014.122919	19.941965
55.850207	2007.785008	19.946983
55.412576	1996.921261	19.952000
55.175982	1991.892545	19.957018
55.352055	1987.587477	19.962035
55.117969	1978.439715	19.967053
55.744805	1979.194035	19.972071
55.827694	1983.671499	19.977088
55.275267	1981.472424	19.982106
55.638202	1987.091076	19.987123
55.367882	1966.639746	19.992141
55.613547	1982.599844	19.997159
55.586613	2001.606249	20.002176
55.774993	2002.106487	20.007194
55.574836	2004.243986	20.012211
55.307996	2016.008575	20.017229
55.598792	2003.149064	20.022247
55.702913	2013.264335	20.027264
55.520392	2010.217404	20.032282
56.143600	2022.532280	20.037299
56.014840	2036.613968	20.042317
56.477140	2036.692211	20.047335
56.361468	2029.029610	20.052352
56.525888	2031.216106	20.057370
56.324336	2034.827892	20.062387
56.609831	2043.721608	20.067405
56.971084	2029.719058	20.072423
56.901606	2025.448456	20.077440
56.729554	2019.776850	20.082458
56.731474	2017.239930	20.087475
57.128279	2028.656894	20.092493
56.824994	2009.972376	20.097511
56.526478	1997.462984	20.102528
56.756861	2019.349006	20.107546
57.187145	2021.358116	20.112563
56.866576	2031.412885	20.117581
56.960918	2033.693434	20.122599
57.060833	2031.198973	20.127616
57.081582	2027.412421	20.132634
57.229835	2029.847428	20.137651
56.980008	2038.164912	20.142669
57.105094	2025.768546	20.147687
57.019548	2027.338153	20.152704
56.954913	2039.496857	20.157722
57.146837	2049.783646	20.162739
57.082886	2064.736249	20.167757
57.312563	2055.628917	20.172775
57.625304	2053.396102	20.177792
57.427972	2069.436187	20.182810
57.796410	2068.319243	20.187827
57.505182	2084.805524	20.192845
57.745553	2088.849360	20.197863
57.749202	2077.153658	20.202880
57.920749	2085.770984	20.207898
58.369242	2085.719436	20.212915
57.788487	2085.749793	20.217933
58.151090	2076.246900	20.222951
58.280851	2088.514449	20.227968
58.354607	2074.766826	20.232986
59.131130	2085.161146	20.238003
58.586609	2084.527317	20.243021
58.543341	2073.883355	20.248039
58.695815	2063.543239	20.253056
58.516049	2073.545046	20.258074
58.870348	2068.012206	20.263091
58.934485	2068.359571	20.268109
58.684720	2057.436786	20.273127
58.799681	2058.947280	20.278144
58.856465	2080.166875	20.283162
59.181090	2081.149076	20.288179
59.242269	2082.628700	20.293197
58.960590	2087.036729	20.298215
59.134607	2084.257995	20.303232
59.050793	2095.165123	20.308250
59.045413	2086.301123	20.313267
59.316359	2089.487634	20.318285
59.076112	2095.091447	20.323303
59.502484	2089.315020	20.328320
59.382558	2085.223783	20.333338
59.412781	2091.172426	20.338355
59.060878	2094.616179	20.343373
59.321827	2091.734111	20.348391
59.658252	2100.522800	20.353408
59.384101	2107.720835	20.358426
59.900142	2116.839460	20.363443
60.013354	2129.776047	20.368461
60.091766	2118.866302	20.373479
60.186241	2120.788217	20.378496
59.919759	2118.758972	20.383514
60.210585	2116.234524	20.388531
60.030367	2122.771638	20.393549
60.183455	2120.755727	20.398567
60.415638	2111.687314	20.403584
60.443890	2124.451538	20.408602
61.027289	2115.271546	20.413619
60.665918	2113.593578	20.418637
60.693751	2115.506428	20.423655
61.174711	2105.675723	20.428672
60.661157	2110.438971	20.433690
60.935238	2123.556231	20.438707
60.765816	2113.416110	20.443725
60.687709	2114.877027	20.448743
60.670183	2114.365144	20.453760
60.620270	2112.991772	20.458778
60.652541	2112.646445	20.463795
60.900095	2123.203392	20.468813
60.798098	2122.734598	20.473831
61.362849	2136.546672	20.478848
61.240165	2149.552963	20.483866
61.289098	2138.639809	20.488883
61.140911	2141.791076	20.493901
61.143015	2141.048411	20.498919
61.431386	2129.166657	20.503936
61.192276	2143.252901	20.508954
61.268071	2145.241088	20.513971
61.393990	2161.898651	20.518989
61.656292	2169.733386	20.524007
61.957616	2175.237302	20.529024
61.753986	2170.822112	20.534042
61.865284	2169.589205	20.539059
61.967606	2172.386120	20.544077
61.906541	2170.839013	20.549095
62.083218	2160.364531	20.554112
62.149047	2159.586928	20.559130
62.303712	2182.624558	20.564147
62.768889	2187.781157	20.569165
62.725940	2183.033339	20.574183
62.803086	2167.821832	20.579200
62.567244	2165.147030	20.584218
62.485199	2149.921693	20.589235
62.602104	2152.319582	20.594253
62.529753	2164.999293	20.599271
62.783262	2173.237806	20.604288
62.929130	2180.410360	20.609306
62.981090	2175.440581	20.614323
62.865097	2184.370806	20.619341
62.941572	2188.680312	20.624359
63.366186	2181.117310	20.629376
62.987876	2184.357395	20.634394
63.291812	2177.134188	20.639411
63.130449	2178.868489	20.644429
63.202006	2183.610849	20.649447
63.278192	2175.596226	20.654464
63.419411	2182.793562	20.659482
63.240762	2186.469112	20.664499
63.375260	2173.858889	20.669517
62.839668	2172.596870	20.674535
63.539270	2195.395270	20.679552
63.161988	2208.404119	20.684570
63.375785	2208.055168	20.689587
63.242705	2216.710309	20.694605
63.279733	2221.443035	20.699623
63.594206	2225.535089	20.704640
63.626620	2238.694351	20.709658
64.085691	2227.741308	20.714675
64.617547	2220.100335	20.719693
64.501926	2220.167793	20.724711
64.778072	2215.649884	20.729728
64.510507	2218.919703	20.734746
64.663837	2206.971237	20.739763
64.806963	2209.048296	20.744781
64.630103	2218.306285	20.749799
64.654895	2206.003507	20.754816
64.578065	2209.197124	20.759834
64.767674	2216.463638	20.764851
64.885105	2217.588738	20.769869
64.514548	2214.022104	20.774887
64.961479	2214.129461	20.779904
65.030302	2238.490288	20.784922
65.028790	2236.686703	20.789939
65.525431	2247.307486	20.794957
65.598376	2248.511980	20.799975
65.434993	2239.425403	20.804992
65.029268	2230.114140	20.810010
65.298456	2241.723595	20.815027
65.638684	2235.195675	20.820045
65.327124	2246.413550	20.825063
65.704741	2243.858599	20.830080
65.437783	2243.974095	20.835098
65.400167	2244.386699	20.840115
65.651739	2236.581228	20.845133
65.346286	2248.756863	20.850151
65.710610	2256.452749	20.855168
65.787389	2265.249206	20.860186
65.928002	2272.570296	20.865203
66.461983	2263.951482	20.870221
66.231850	2266.977746	20.875239
65.986495	2277.593420	20.880256
66.048610	2275.105757	20.885274
66.199431	2266.800629	20.890291
66.253512	2283.028306	20.895309
66.261439	2296.756376	20.900327
66.579327	2290.736999	20.905344
66.598827	2295.704118	20.910362
66.283305	2299.841052	20.915379
66.744713	2290.783470	20.920397
66.426294	2295.639713	20.925415
66.669596	2293.826963	20.930432
67.026348	2313.158895	20.935450
67.381655	2310.112783	20.940467
67.350594	2294.370263	20.945485
67.372007	2319.412613	20.950503
67.624841	2303.797957	20.955520
67.571623	2299.451764	20.960538
67.491539	2310.125181	20.965555
67.892501	2302.040879	20.970573
67.479249	2289.768299	20.975591
67.868223	2279.744435	20.980608
67.922406	2273.163580	20.985626
67.632418	2279.449830	20.990643
67.623294	2264.770546	20.995661
67.372787	2283.507776	21.000679
68.215783	2294.396327	21.005696
68.227194	2303.164438	21.010714
68.226535	2295.601781	21.015731
68.200478	2304.504420	21.020749
67.936872	2300.011907	21.025767
68.205013	2310.342964	21.030784
68.237852	2299.886054	21.035802
68.058209	2289.904578	21.040819
68.105296	2294.554963	21.045837
67.904077	2302.905497	21.050855
68.200653	2323.119353	21.055872
68.241601	2326.860017	21.060890
68.373130	2325.613125	21.065907
68.681730	2329.523714	21.070925
68.483986	2340.267378	21.075943
68.535016	2334.794400	21.080960
68.925658	2355.111248	21.085978
68.805113	2364.072051	21.090995
69.080808	2359.131771	21.096013
68.960214	2364.177373	21.101031
69.086125	2359.478164	21.106048
69.187135	2352.462606	21.111066
69.086263	2358.897345	21.116083
69.134010	2374.032756	21.121101
69.500659	2383.004392	21.126119
69.913366	2382.020060	21.131136
70.099752	2390.031417	21.136154
70.124466	2402.574230	21.141171
70.420013	2378.725579	21.146189
70.327556	2379.107685	21.151207
70.256591	2356.820292	21.156224
70.379994	2351.932934	21.161242
70.271003	2344.662540	21.166259
70.163940	2340.852155	21.171277
70.091126	2348.168395	21.176295
70.485572	2363.845074	21.181312
70.578625	2370.961293	21.186330
70.285650	2381.926217	21.191347
70.452083	2376.297355	21.196365
70.420114	2371.502195	21.201383
70.435876	2377.507271	21.206400
70.698934	2380.069610	21.211418
70.341618	2374.610558	21.216435
70.575812	2381.819196	21.221453
70.731119	2389.219008	21.226471
70.579359	2400.003930	21.231488
70.767870	2401.766258	21.236506
70.832471	2404.767858	21.241523
71.224899	2405.795762	21.246541
71.168478	2406.141405	21.251559
71.425448	2420.323271	21.256576
71.729158	2430.375522	21.261594
71.637428	2429.816249	21.266611
71.742290	2429.570524	21.271629
71.824938	2422.779209	21.276647
71.850918	2418.089411	21.281664
71.888890	2419.320759	21.286682
71.695294	2424.092641	21.291699
71.908824	2429.747956	21.296717
71.821164	2426.371905	21.301735
71.748262	2419.780298	21.306752
72.014299	2418.311386	21.311770
72.100720	2427.500207	21.316787
72.340432	2425.874043	21.321805
72.086600	2434.163072	21.326823
72.281418	2445.675532	21.331840
72.755070	2433.407444	21.336858
72.476757	2459.802790	21.341875
72.807732	2436.365485	21.346893
72.690698	2445.586167	21.351911
72.832087	2451.102833	21.356928
72.781992	2440.268030	21.361946
73.016595	2441.437755	21.366963
72.981114	2436.059542	21.371981
72.857962	2436.363068	21.376999
73.119107	2452.678547	21.382016
73.093687	2433.492910	21.387034
72.486320	2441.540980	21.392051
73.259895	2463.361492	21.397069
73.127876	2470.557269	21.402087
73.293442	2472.148609	21.407104
73.488209	2471.933495	21.412122
73.372128	2488.964249	21.417139
73.542147	2475.033447	21.422157
73.613322	2482.436184	21.427175
73.495631	2485.790929	21.432192
74.000176	2498.354127	21.437210
73.930435	2488.726773	21.442227
74.097369	2493.191875	21.447245
74.040948	2501.512289	21.452263
74.002172	2501.446783	21.457280
74.199834	2504.983654	21.462298
74.143253	2521.364700	21.467315
74.487641	2530.418639	21.472333
74.679218	2523.870677	21.477351
74.708671	2520.461081	21.482368
74.902539	2514.751263	21.487386
74.653790	2523.310345	21.492403
74.851880	2529.073358	21.497421
75.011544	2530.195439	21.502439
74.959911	2525.198969	21.507456
75.363826	2514.102096	21.512474
75.154931	2517.638442	21.517491
75.383865	2516.393351	21.522509
75.461196	2513.673035	21.527527
75.606846	2521.032384	21.532544
75.432303	2502.833434	21.537562
75.291151	2524.342038	21.542579
75.400189	2542.503671	21.547597
75.874799	2541.240027	21.552615
75.987226	2557.935874	21.557632
75.905117	2546.145532	21.562650
75.946467	2547.046042	21.567667
75.974049	2538.015914	21.572685
75.877824	2545.698490	21.577703
76.236838	2535.947307	21.582720
76.300301	2529.029598	21.587738
76.342270	2528.035465	21.592755
76.329806	2534.051367	21.597773
76.344234	2526.920913	21.602791
76.139510	2531.315366	21.607808
76.495670	2539.131041	21.612826
76.657885	2555.058086	21.617843
77.018429	2554.637441	21.622861
77.038743	2561.404574	21.627879
77.022831	2564.666932	21.632896
77.265327	2549.260416	21.637914
77.343629	2558.790199	21.642931
77.115199	2554.267390	21.647949
77.415159	2556.136311	21.652967
77.194451	2560.496407	21.657984
77.217192	2553.694661	21.663002
77.099183	2550.348793	21.668019
77.099667	2556.051171	21.673037
77.380877	2551.389032	21.678055
77.261505	2545.640224	21.683072
77.695309	2554.518783	21.688090
77.557791	2573.072744	21.693107
77.397208	2574.243024	21.698125
77.755564	2576.979989	21.703143
77.580105	2580.107704	21.708160
77.619147	2581.475689	21.713178
78.038733	2593.710511	21.718195
77.872273	2601.390351	21.723213
78.024835	2610.725231	21.728231
78.453148	2611.812766	21.733248
78.629148	2599.199669	21.738266
78.631083	2599.352615	21.743283
78.260977	2596.174174	21.748301
78.479852	2595.816896	21.753319
78.736335	2622.402472	21.758336
78.742283	2627.483741	21.763354
78.918264	2631.810193	21.768371
79.407299	2619.235502	21.773389
79.678991	2614.960716	21.778407
79.526003	2617.224156	21.783424
79.772715	2612.984599	21.788442
79.611004	2623.678414	21.793459
79.186535	2619.581654	21.798477
79.981433	2611.853719	21.803495
79.869349	2617.715459	21.808512
79.831399	2616.236333	21.813530
79.552999	2606.211920	21.818547
79.996815	2621.788191	21.823565
79.723021	2613.718190	21.828583
79.874122	2619.526008	21.833600
80.028465	2615.476505	21.838618
79.974518	2617.333054	21.843635
79.763802	2627.288959	21.848653
79.919842	2637.580104	21.853671
79.914477	2656.452460	21.858688
80.384570	2653.436524	21.863706
80.629092	2654.909724	21.868723
80.397435	2653.515356	21.873741
80.501617	2654.308843	21.878759
80.203830	2671.582211	21.883776
80.256704	2675.764660	21.888794
80.585518	2679.555471	21.893811
80.747946	2675.223139	21.898829
80.841624	2697.516942	21.903847
80.747548	2709.598170	21.908864
81.310587	2705.205142	21.913882
81.738658	2707.309194	21.918899
81.960749	2697.461252	21.923917
82.196368	2691.047665	21.928935
82.166673	2705.140953	21.933952
82.191294	2696.130119	21.938970
82.294812	2690.432214	21.943987
81.755937	2687.193065	21.949005
81.919948	2679.188076	21.954023
82.018939	2689.282987	21.959040
81.937173	2685.744105	21.964058
82.099741	2683.593887	21.969075
82.295837	2693.986514	21.974093
82.126005	2689.857892	21.979111
81.930412	2686.788183	21.984128
81.937763	2689.264492	21.989146
82.278171	2698.788448	21.994163
82.252833	2710.587864	21.999181
82.743320	2716.729374	22.004199
82.586984	2716.402602	22.009216
82.583770	2727.229342	22.014234
82.584536	2740.801323	22.019251
82.998520	2749.416358	22.024269
83.228361	2749.845012	22.029287
83.348258	2757.304786	22.034304
83.171676	2752.234408	22.039322
83.380435	2750.940274	22.044339
83.144176	2745.184133	22.049357
83.537303	2741.367170	22.054375
83.380487	2750.542248	22.059392
83.748387	2746.178698	22.064410
83.867624	2763.094299	22.069427
83.917008	2767.301363	22.074445
84.230333	2755.481144	22.079463
84.062316	2774.766523	22.084480
83.880929	2766.762465	22.089498
84.141854	2753.442731	22.094515
84.129733	2761.968747	22.099533
84.256163	2756.979390	22.104551
84.293936	2764.418882	22.109568
84.569871	2773.829531	22.114586
84.784193	2791.074704	22.119603
84.482243	2796.615742	22.124621
84.880315	2802.063151	22.129639
85.081396	2788.951689	22.134656
84.890233	2792.567445	22.139674
84.758903	2796.153631	22.144691
84.853590	2794.902751	22.149709
85.259158	2790.591229	22.154727
85.188773	2792.620585	22.159744
84.880149	2814.017313	22.164762
85.408355	2824.607495	22.169779
85.267590	2827.489382	22.174797
85.688595	2826.434563	22.179815
85.517745	2823.524114	22.184832
85.790695	2823.581101	22.189850
86.074883	2853.838074	22.194867
86.081228	2851.138090	22.199885
86.556436	2844.706895	22.204903
86.760436	2849.034487	22.209920
86.698763	2833.077985	22.214938
86.972449	2817.342444	22.219955
86.626872	2813.987669	22.224973
86.960703	2796.792294	22.229991
86.478805	2810.594480	22.235008
86.648102	2806.552298	22.240026
86.740379	2810.231057	22.245043
86.403970	2832.875638	22.250061
86.719498	2831.764630	22.255079
86.778517	2836.691340	22.260096
86.858218	2838.204589	22.265114
87.090244	2843.788501	22.270131
87.337695	2849.454901	22.275149
87.396311	2863.928009	22.280167
87.269159	2871.392838	22.285184
87.333863	2868.503690	22.290202
87.605881	2866.625896	22.295219
87.563340	2875.768779	22.300237
87.659514	2862.216741	22.305255
87.586513	2868.367967	22.310272
87.697952	2894.710869	22.315290
87.978565	2894.331179	22.320307
88.117552	2896.326738	22.325325
88.129554	2894.469468	22.330343
88.123514	2898.249923	22.335360
88.539168	2902.280757	22.340378
88.681469	2910.744331	22.345395
88.396478	2916.586530	22.350413
88.569586	2919.538609	22.355431
88.872397	2917.438409	22.360448
88.872767	2914.536656	22.365466
89.348319	2913.499588	22.370483
89.294337	2915.883711	22.375501
89.128703	2907.139614	22.380519
89.375736	2914.560346	22.385536
89.430110	2916.635240	22.390554
89.642267	2902.385690	22.395571
89.391695	2911.921220	22.400589
89.735200	2917.413512	22.405607
89.755676	2903.196029	22.410624
89.438773	2910.318236	22.415642
89.533065	2899.297842	22.420659
89.713466	2909.071980	22.425677
89.841702	2927.996407	22.430695
89.600737	2935.261187	22.435712
89.604894	2941.781169	22.440730
90.002979	2930.473556	22.445747
90.230641	2936.292857	22.450765
90.031672	2958.268878	22.455783
90.117713	2957.518209	22.460800
90.280545	2959.447634	22.465818
90.546397	2951.760895	22.470835
90.806445	2958.773219	22.475853
91.091959	2961.185890	22.480871
91.396510	2957.254778	22.485888
91.228511	2969.162803	22.490906
91.582644	2969.088664	22.495923
91.505247	2969.133076	22.500941
91.571395	2965.016564	22.505959
91.635023	2971.100767	22.510976
91.647950	2967.523733	22.515994
91.696029	2969.563455	22.521011
91.827353	2975.675449	22.526029
91.867177	2962.618832	22.531047
92.066572	2960.530204	22.536064
91.931665	2974.474005	22.541082
92.319602	2967.382804	22.546099
92.006429	2966.452446	22.551117
91.725179	2968.213140	22.556135
92.354196	2980.705577	22.561152
92.209183	2999.111885	22.566170
92.556830	3000.571031	22.571187
92.474842	3000.711079	22.576205
92.371102	3003.969540	22.581223
92.874911	3011.032942	22.586240
92.756987	3023.338621	22.591258
92.971463	3032.867060	22.596275
93.018757	3027.161197	22.601293
92.838783	3031.360960	22.606311
93.075386	3025.393904	22.611328
93.463740	3045.119154	22.616346
93.768188	3049.008175	22.621363
93.867242	3055.031048	22.626381
93.518075	3053.265329	22.631399
93.966160	3045.516543	22.636416
93.916282	3053.168681	22.641434
93.898787	3051.647749	22.646451
93.996170	3041.532610	22.651469
93.860826	3041.616517	22.656487
94.265564	3052.955182	22.661504
94.267190	3070.808625	22.666522
94.333592	3062.479228	22.671539
94.357361	3076.303203	22.676557
94.391117	3087.759099	22.681575
94.728887	3072.915430	22.686592
94.536405	3084.736254	22.691610
94.803057	3071.858590	22.696627
94.555804	3069.172522	22.701645
94.482090	3095.388100	22.706663
94.943758	3101.369180	22.711680
94.837982	3100.850587	22.716698
94.994421	3102.101979	22.721715
95.372654	3111.319166	22.726733
95.679715	3127.051022	22.731751
95.850140	3125.941139	22.736768
95.918854	3135.492547	22.741786
96.194822	3119.989779	22.746803
95.754481	3129.027292	22.751821
95.511342	3133.350509	22.756839
96.280422	3128.475695	22.761856
96.053341	3123.785572	22.766874
95.602271	3133.920884	22.771891
95.841433	3135.251912	22.776909
96.114732	3147.250137	22.781927
96.396367	3155.873099	22.786944
96.326691	3159.216511	22.791962
96.864520	3182.087990	22.796979
96.966351	3186.777824	22.801997
96.838168	3190.369485	22.807015
97.092776	3182.659689	22.812032
96.904853	3178.473691	22.817050
97.210632	3188.653651	22.822067
97.165289	3185.604682	22.827085
97.781506	3200.130447	22.832103
97.786498	3202.352905	22.837120
97.550255	3210.105600	22.842138
97.739768	3206.085564	22.847155
97.995976	3210.636120	22.852173
97.923100	3200.794279	22.857191
98.103116	3199.677295	22.862208
98.219667	3205.041451	22.867226
98.284807	3192.404853	22.872243
98.240714	3194.481095	22.877261
98.060653	3212.209218	22.882279
98.698677	3207.421783	22.887296
98.792560	3220.644556	22.892314
99.034501	3220.963354	22.897331
98.988127	3221.072323	22.902349
99.036355	3236.930918	22.907367
99.412966	3221.812980	22.912384
99.474076	3216.237831	22.917402
99.275580	3229.345152	22.922419
99.326236	3211.207560	22.927437
99.385716	3217.518129	22.932455
99.295835	3220.355854	22.937472
99.269763	3235.499190	22.942490
99.398049	3239.520515	22.947507
99.759812	3251.847107	22.952525
99.458092	3245.190992	22.957543
100.204897	3261.327471	22.962560
99.887054	3273.993541	22.967578
100.088108	3278.022930	22.972595
100.354051	3283.943514	22.977613
100.154988	3284.982413	22.982631
100.721226	3264.191129	22.987648
100.677203	3279.564633	22.992666
100.570451	3283.231906	22.997683
100.851677	3284.188684	23.002701
100.954585	3298.420241	23.007719
101.087187	3300.372814	23.012736
101.332822	3302.439383	23.017754
100.898677	3306.856413	23.022771
101.176616	3299.869456	23.027789
101.538717	3299.084177	23.032807
101.888974	3292.309283	23.037824
101.667675	3300.865831	23.042842
101.722863	3300.118276	23.047859
102.188021	3293.341717	23.052877
101.719848	3295.856544	23.057895
102.156755	3303.640567	23.062912
102.136148	3322.949511	23.067930
102.207128	3329.388931	23.072947
102.396071	3319.539183	23.077965
102.272637	3332.364903	23.082983
102.532129	3325.087289	23.088000
102.703436	3316.108153	23.093018
102.633804	3319.380728	23.098035
102.835031	3322.194383	23.103053
102.830878	3318.806306	23.108071
103.267987	3321.821921	23.113088
103.195253	3343.995734	23.118106
103.346951	3335.526507	23.123123
103.599424	3329.631514	23.128141
103.287019	3334.207958	23.133159
103.326589	3332.868902	23.138176
103.228713	3329.148287	23.143194
103.304462	3336.342021	23.148211
103.810449	3359.304456	23.153229
103.667284	3364.204509	23.158247
103.835146	3368.266572	23.163264
103.842445	3366.674977	23.168282
103.421434	3376.393676	23.173299
104.024623	3385.162446	23.178317
104.224234	3398.885606	23.183335
104.206584	3404.457437	23.188352
104.491433	3418.444477	23.193370
104.544492	3438.635469	23.198387
104.510962	3422.790636	23.203405
104.618034	3431.356379	23.208423
105.313691	3443.004732	23.213440
105.310997	3445.065506	23.218458
105.630941	3445.454883	23.223475
105.902669	3440.869636	23.228493
105.877750	3436.870408	23.233511
105.857891	3428.555856	23.238528
106.153762	3433.666055	23.243546
106.116345	3438.711253	23.248563
106.508463	3436.343083	23.253581
106.105546	3435.870429	23.258599
106.175522	3430.270905	23.263616
106.701098	3433.938054	23.268634
106.496542	3441.693108	23.273651
106.703856	3428.908416	23.278669
106.603152	3424.044959	23.283687
106.674775	3434.140942	23.288704
106.507202	3425.594506	23.293722
106.805797	3437.110439	23.298739
107.043027	3450.649479	23.303757
106.907862	3449.008978	23.308775
107.091597	3453.759767	23.313792
107.343751	3450.908826	23.318810
107.217042	3460.393909	23.323827
107.254284	3471.519204	23.328845
107.332598	3484.243995	23.333863
107.510807	3473.751051	23.338880
107.982635	3486.095075	23.343898
107.908484	3497.009271	23.348915
108.061333	3508.983981	23.353933
107.883407	3518.355123	23.358951
108.350367	3514.300186	23.363968
108.415357	3510.510882	23.368986
108.647069	3510.072332	23.374003
108.899540	3495.415976	23.379021
109.071843	3498.342315	23.384039
109.233178	3494.907169	23.389056
108.942247	3490.868420	23.394074
108.858890	3501.368004	23.399091
109.164440	3494.055536	23.404109
108.835548	3509.233430	23.409127
108.860373	3523.057235	23.414144
109.546349	3528.815200	23.419162
109.481845	3529.899596	23.424179
109.787909	3522.607109	23.429197
109.595773	3528.293643	23.434215
109.831051	3558.039217	23.439232
109.899305	3559.359156	23.444250
109.598588	3566.795125	23.449267
109.916564	3565.550594	23.454285
109.690161	3576.878977	23.459303
109.858807	3588.857831	23.464320
109.881663	3596.090348	23.469338
110.329882	3614.215106	23.474355
110.398149	3617.909836	23.479373
110.423805	3621.537592	23.484391
110.970336	3625.868645	23.489408
111.438154	3632.175293	23.494426
111.710251	3649.385106	23.499443
112.215573	3635.413605	23.504461
112.049458	3627.362483	23.509479
111.780706	3614.446071	23.514496
111.903433	3602.808278	23.519514
111.944183	3607.024478	23.524531
112.264383	3624.759776	23.529549
112.073825	3625.656347	23.534567
112.057629	3644.025597	23.539584
112.192789	3640.360100	23.544602
112.165766	3645.292230	23.549619
112.580720	3634.516752	23.554637
112.146616	3642.976762	23.559655
112.359243	3659.333818	23.564672
113.032853	3661.988376	23.569690
112.786289	3677.846134	23.574707
113.026981	3666.682895	23.579725
113.016399	3681.333949	23.584743
112.887779	3686.525006	23.589760
113.159692	3690.613268	23.594778
113.418518	3695.380463	23.599795
113.542757	3696.774627	23.604813
113.262854	3699.313130	23.609831
113.373043	3721.834420	23.614848
113.919831	3717.332382	23.619866
114.110282	3729.154592	23.624883
114.171692	3730.633944	23.629901
114.421477	3729.793976	23.634919
114.554180	3732.885960	23.639936
114.478109	3743.512456	23.644954
114.485424	3748.918474	23.649971
114.672982	3741.188379	23.654989
114.790195	3745.888046	23.660007
114.858276	3757.206875	23.665024
115.033888	3755.448451	23.670042
115.214138	3765.653079	23.675059
115.572349	3768.892058	23.680077
115.948628	3765.501257	23.685095
115.451331	3776.977304	23.690112
115.804277	3761.065901	23.695130
115.985945	3772.793926	23.700147
115.918079	3771.307230	23.705165
115.819164	3766.117778	23.710183
116.036497	3757.957163	23.715200
116.107822	3758.458498	23.720218
115.830524	3778.586806	23.725235
116.362434	3775.734854	23.730253
116.480891	3783.977256	23.735271
116.266669	3790.242340	23.740288
116.862721	3788.509715	23.745306
116.229574	3802.347611	23.750323
116.517148	3813.035326	23.755341
116.768173	3810.800258	23.760359
116.958216	3835.532548	23.765376
117.334456	3844.974128	23.770394
117.629405	3843.532986	23.775411
117.848025	3846.672213	23.780429
118.006304	3836.868544	23.785447
117.760084	3843.896818	23.790464
118.097314	3840.951433	23.795482
117.882001	3836.578441	23.800499
117.940415	3855.046636	23.805517
118.094123	3868.287636	23.810535
117.826835	3864.787407	23.815552
118.555021	3867.927083	23.820570
118.627334	3892.945456	23.825587
118.716733	3900.852954	23.830605
118.636668	3896.464290	23.835623
118.842381	3894.585521	23.840640
119.264680	3890.579601	23.845658
119.546657	3893.158361	23.850675
119.209646	3907.683252	23.855693
119.682160	3911.218339	23.860711
119.846443	3929.025025	23.865728
120.119467	3918.999192	23.870746
120.048918	3920.299184	23.875763
120.192464	3919.575976	23.880781
120.517662	3922.101536	23.885799
120.244198	3909.919130	23.890816
120.360173	3918.575011	23.895834
120.224784	3926.194464	23.900851
120.121091	3932.709850	23.905869
120.649955	3942.951478	23.910887
120.465001	3949.226751	23.915904
120.808416	3933.567538	23.920922
120.830274	3966.253140	23.925939
120.978167	3970.753708	23.930957
121.398927	3978.504126	23.935975
121.476630	3978.281568	23.940992
121.475095	3976.829956	23.946010
121.286601	3990.703206	23.951027
121.637112	4002.755874	23.956045
122.312641	3999.366362	23.961063
122.062032	4011.439232	23.966080
122.231651	4002.493051	23.971098
122.399734	4006.568238	23.976115
122.295146	4011.244005	23.981133
122.547821	4012.427207	23.986151
122.332880	4037.802341	23.991168
122.516325	4027.697537	23.996186
122.621348	4034.118239	24.001203
123.112575	4049.691073	24.006221
123.122841	4057.968820	24.011239
123.031220	4065.021254	24.016256
123.275945	4057.504397	24.021274
123.369001	4052.054382	24.026291
123.555802	4078.360463	24.031309
123.762391	4087.132964	24.036327
123.852711	4085.190562	24.041344
123.667733	4083.038525	24.046362
123.747332	4087.127174	24.051379
124.108896	4095.687059	24.056397
124.458166	4100.850863	24.061415
124.444605	4113.790569	24.066432
124.631357	4110.009741	24.071450
124.924399	4109.562617	24.076467
124.740530	4115.944079	24.081485
125.042237	4092.952432	24.086503
125.341634	4109.529096	24.091520
125.218500	4112.618153	24.096538
125.609711	4118.235675	24.101555
125.682668	4135.899811	24.106573
125.810048	4141.005409	24.111591
125.581890	4137.088011	24.116608
125.917474	4135.862969	24.121626
125.882885	4122.890510	24.126643
125.808717	4124.562780	24.131661
126.174481	4136.659883	24.136679
125.947890	4151.273843	24.141696
126.227628	4155.346368	24.146714
126.642347	4152.161737	24.151731
126.537565	4147.072735	24.156749
126.764348	4162.279919	24.161767
126.662906	4182.932068	24.166784
126.955844	4174.189828	24.171802
127.364284	4178.605276	24.176819
127.158816	4183.555252	24.181837
127.729219	4196.644210	24.186855
127.445667	4214.092533	24.191872
127.519117	4209.944957	24.196890
127.684604	4208.385407	24.201907
127.994653	4220.161063	24.206925
128.239107	4227.588366	24.211943
128.156240	4236.055226	24.216960
128.384643	4236.999929	24.221978
128.513827	4234.429018	24.226995
128.552017	4238.221782	24.232013
128.559448	4253.509397	24.237031
128.808389	4266.426721	24.242048
128.965037	4260.866516	24.247066
129.336055	4269.800933	24.252083
129.060598	4268.756380	24.257101
129.343773	4279.598693	24.262119
129.559589	4294.671593	24.267136
130.019738	4296.717026	24.272154
129.785859	4296.032150	24.277171
129.852541	4292.404588	24.282189
130.124427	4296.574908	24.287207
130.348838	4300.699529	24.292224
130.115686	4324.447761	24.297242
130.741889	4320.837191	24.302259
130.722567	4326.546248	24.307277
131.021342	4315.672172	24.312295
130.801333	4320.143866	24.317312
130.957156	4327.804769	24.322330
130.940345	4324.282338	24.327347
130.922792	4352.527844	24.332365
131.125819	4351.709352	24.337383
131.007239	4350.765255	24.342400
130.913687	4368.397717	24.347418
131.361668	4368.456503	24.352435
131.858730	4369.641086	24.357453
132.064960	4394.613727	24.362471
132.390024	4399.133571	24.367488
132.578511	4403.749216	24.372506
132.715687	4408.545396	24.377523
132.510108	4411.259142	24.382541
132.842721	4401.310166	24.387559
132.857580	4404.863508	24.392576
132.883516	4400.092996	24.397594
133.123572	4405.735600	24.402611
133.019579	4436.313755	24.407629
133.568237	4420.137835	24.412647
133.428769	4422.750891	24.417664
133.489423	4421.396052	24.422682
133.709095	4421.855967	24.427699
133.314790	4434.729321	24.432717
133.541964	4451.591524	24.437735
133.680230	4452.024732	24.442752
133.772753	4457.285808	24.447770
134.331151	4482.853580	24.452787
134.679366	4481.510672	24.457805
134.706862	4470.386418	24.462823
134.808441	4480.600185	24.467840
134.677064	4481.007867	24.472858
135.248332	4487.878512	24.477875
135.254449	4514.094314	24.482893
135.275727	4512.232563	24.487911
135.829522	4516.374078	24.492928
135.415156	4510.158886	24.497946
135.757517	4497.738426	24.502963
136.085490	4515.257306	24.507981
136.282300	4524.665955	24.512999
136.417923	4532.936234	24.518016
136.194780	4533.846902	24.523034
136.671182	4528.849546	24.528051
136.770513	4533.694540	24.533069
136.819132	4534.935519	24.538087
136.921192	4525.908859	24.543104
136.500540	4538.471674	24.548122
137.148610	4548.527858	24.553139
137.187491	4556.862169	24.558157
136.990375	4553.289948	24.563175
137.621052	4566.240119	24.568192
137.155973	4573.813573	24.573210
137.702395	4580.358425	24.578227
137.518001	4590.864020	24.583245
137.751753	4599.525623	24.588263
137.994308	4604.744240	24.593280
137.997769	4608.331404	24.598298
137.842491	4622.124131	24.603315
138.305830	4634.215344	24.608333
138.682696	4633.204323	24.613351
138.643012	4647.417368	24.618368
139.316493	4658.247818	24.623386
139.578103	4653.272922	24.628403
139.483344	4671.770546	24.633421
139.507568	4658.422940	24.638439
139.714917	4662.243371	24.643456
139.930823	4672.251747	24.648474
140.096338	4667.795906	24.653491
140.410718	4685.972776	24.658509
140.471691	4682.542536	24.663527
140.681515	4690.436443	24.668544
140.548785	4690.171476	24.673562
140.635423	4675.467001	24.678579
140.689593	4682.344826	24.683597
140.843771	4693.950129	24.688615
141.204247	4699.585935	24.693632
140.882069	4713.278360	24.698650
141.245543	4708.625219	24.703667
141.347394	4719.232430	24.708685
141.346107	4731.450102	24.713703
141.879189	4740.511566	24.718720
141.450596	4749.285453	24.723738
141.835060	4737.890593	24.728755
141.675237	4755.532080	24.733773
141.957464	4761.620632	24.738791
142.027480	4768.590765	24.743808
142.037876	4777.312211	24.748826
142.683939	4781.184992	24.753843
142.760503	4793.715461	24.758861
142.916177	4796.353831	24.763879
143.405043	4785.109806	24.768896
143.461554	4788.122852	24.773914
143.792847	4794.410804	24.778931
143.886425	4786.749663	24.783949
143.538385	4776.574707	24.788967
144.144356	4798.106122	24.793984
144.000809	4812.472709	24.799002
144.106179	4804.661569	24.804019
144.312474	4826.368522	24.809037
144.197102	4814.006122	24.814055
144.436144	4815.942482	24.819072
144.192860	4833.147816	24.824090
144.532871	4833.411076	24.829107
144.662361	4844.919776	24.834125
144.560517	4860.102017	24.839143
144.911238	4866.165118	24.844160
145.533537	4871.585664	24.849178
145.811354	4875.906353	24.854195
145.361729	4881.418585	24.859213
145.221236	4898.976720	24.864231
145.958820	4898.431710	24.869248
146.287367	4911.761647	24.874266
146.438968	4933.981762	24.879283
146.488110	4938.265840	24.884301
146.360103	4948.077263	24.889319
146.623719	4938.483470	24.894336
146.773005	4947.772265	24.899354
146.952207	4965.682405	24.904371
147.367325	4975.696645	24.909389
147.102606	4964.401409	24.914407
147.474784	4964.777476	24.919424
147.428380	4984.700666	24.924442
147.870746	4983.119308	24.929459
148.022852	4993.723914	24.934477
148.023398	4990.396512	24.939495
148.195756	4999.045646	24.944512
148.472234	5012.106691	24.949530
148.697167	5010.210441	24.954547
148.405536	5010.478854	24.959565
148.782044	5011.161319	24.964583
149.147126	5014.313988	24.969600
149.093133	5043.182565	24.974618
148.973888	5047.376376	24.979635
149.609714	5033.600984	24.984653
149.323075	5036.358941	24.989671
149.657025	5057.632489	24.994688
149.657917	5064.952788	24.999706
150.013371	5064.818585	25.004723
149.754331	5069.174095	25.009741
149.771290	5082.318635	25.014759
150.386735	5081.230368	25.019776
150.334907	5093.730320	25.024794
150.802908	5094.819362	25.029811
150.885606	5118.813094	25.034829
150.869665	5116.840874	25.039847
151.063996	5119.977681	25.044864
151.270639	5135.104885	25.049882
151.467008	5141.697188	25.054899
151.858535	5137.511377	25.059917
151.761470	5160.131991	25.064935
152.100653	5139.326913	25.069952
151.976213	5150.750227	25.074970
152.140359	5178.234065	25.079987
152.474011	5170.599216	25.085005
152.287522	5179.149462	25.090023
152.600944	5174.392241	25.095040
152.365719	5193.735817	25.100058
152.871987	5209.159679	25.105075
153.213692	5214.065633	25.110093
153.198574	5207.494791	25.115111
153.667197	5205.259405	25.120128
153.836019	5217.359970	25.125146
153.264154	5229.599469	25.130163
153.524504	5239.654809	25.135181
153.546480	5240.887647	25.140199
153.868792	5263.847029	25.145216
153.993110	5269.475603	25.150234
154.152665	5279.337760	25.155251
154.702340	5302.904971	25.160269
154.697634	5306.575936	25.165287
154.770388	5304.457921	25.170304
155.096583	5307.810798	25.175322
154.998589	5308.211802	25.180339
155.472130	5311.302119	25.185357
155.615004	5331.595698	25.190375
156.074914	5314.318448	25.195392
156.182281	5318.656795	25.200410
156.484640	5336.260761	25.205427
156.905516	5336.468539	25.210445
156.523785	5342.020504	25.215463
156.902844	5328.332169	25.220480
157.024240	5331.207420	25.225498
156.992750	5337.950854	25.230515
157.412826	5332.029780	25.235533
157.093591	5330.362005	25.240551
157.439494	5341.531738	25.245568
157.738307	5363.392672	25.250586
157.632303	5356.454461	25.255603
157.880804	5360.370245	25.260621
158.183055	5364.733890	25.265639
158.200572	5363.306169	25.270656
158.561034	5384.823446	25.275674
158.585433	5391.644292	25.280691
158.866045	5384.100790	25.285709
158.774451	5396.830808	25.290727
158.783032	5393.938654	25.295744
159.048310	5407.712981	25.300762
159.139724	5413.399807	25.305779
159.333918	5415.320816	25.310797
159.226723	5422.636305	25.315815
159.489551	5431.984590	25.320832
159.764664	5431.020260	25.325850
159.845160	5432.977383	25.330867
160.082294	5452.044780	25.335885
159.973339	5467.772546	25.340903
160.332751	5471.092802	25.345920
160.206648	5473.853839	25.350938
160.587263	5498.044230	25.355955
160.684464	5498.316124	25.360973
160.896187	5517.738234	25.365991
161.335854	5520.778673	25.371008
161.685740	5516.826441	25.376026
161.620813	5523.947964	25.381043
161.920359	5538.486126	25.386061
162.100925	5549.886895	25.391079
162.255054	5543.080048	25.396096
162.175875	5543.540556	25.401114
162.027915	5552.759128	25.406131
162.789252	5568.375086	25.411149
162.716489	5574.438352	25.416167
162.850053	5582.510687	25.421184
163.171025	5583.423643	25.426202
162.919555	5591.761989	25.431219
163.541069	5604.539326	25.436237
162.965980	5617.462812	25.441255
163.341931	5619.677082	25.446272
163.354016	5633.186320	25.451290
163.702799	5644.161676	25.456307
163.757451	5643.297549	25.461325
163.957235	5671.395340	25.466343
164.442910	5670.027260	25.471360
164.757938	5676.120989	25.476378
164.699121	5684.038526	25.481395
164.962994	5688.145578	25.486413
164.813570	5700.854685	25.491431
165.242070	5695.608548	25.496448
165.508236	5713.163007	25.501466
165.508297	5727.969362	25.506483
166.404309	5719.140397	25.511501
166.327328	5719.461158	25.516519
166.424455	5711.070539	25.521536
166.477843	5720.423284	25.526554
166.729842	5745.238537	25.531571
166.659699	5744.456056	25.536589
166.854721	5758.864430	25.541607
166.733790	5760.326855	25.546624
166.905287	5761.850818	25.551642
167.364986	5785.805329	25.556659
167.628376	5776.282332	25.561677
167.403905	5782.814112	25.566695
167.560733	5813.907448	25.571712
167.899476	5816.802396	25.576730
168.052908	5822.073950	25.581747
168.234249	5840.132397	25.586765
168.584301	5851.755809	25.591783
168.604808	5843.086402	25.596800
169.131828	5865.933700	25.601818
168.890080	5883.473442	25.606835
169.376129	5871.662102	25.611853
169.418595	5881.442397	25.616871
169.354492	5886.832606	25.621888
170.008196	5889.344770	25.626906
169.897776	5900.897040	25.631923
169.991965	5897.439783	25.636941
170.091766	5898.730297	25.641959
170.423379	5918.820592	25.646976
171.153588	5924.510731	25.651994
170.873856	5928.878952	25.657011
171.430006	5916.382672	25.662029
171.169580	5920.233456	25.667047
171.385655	5930.527299	25.672064
171.627611	5930.821747	25.677082
171.524615	5944.374287	25.682100
171.744095	5942.806828	25.687117
172.058354	5965.410647	25.692135
172.135269	5980.943625	25.697152
172.225207	5967.008764	25.702170
171.887896	5984.704981	25.707188
172.751747	5992.888389	25.712205
172.659123	6010.680445	25.717223
172.968827	6010.018286	25.722240
173.110102	6015.358065	25.727258
173.238972	6038.376537	25.732276
173.383299	6033.985237	25.737293
173.514958	6041.444253	25.742311
173.511107	6064.094082	25.747328
173.934629	6063.230409	25.752346
173.700944	6083.708462	25.757364
174.020389	6097.024772	25.762381
174.169575	6089.263636	25.767399
174.115675	6105.211325	25.772416
174.192859	6121.935920	25.777434
174.773031	6136.753516	25.782452
175.030533	6144.949385	25.787469
175.285392	6159.226175	25.792487
175.250214	6161.654542	25.797504
175.778087	6162.489640	25.802522
175.767801	6193.931078	25.807540
175.822049	6180.275985	25.812557
176.047426	6192.609337	25.817575
176.111331	6210.616738	25.822592
176.349180	6212.195147	25.827610
176.673303	6220.665921	25.832628
176.748323	6239.872499	25.837645
176.997256	6257.385527	25.842663
177.091068	6259.294089	25.847680
177.872952	6267.671926	25.852698
177.662297	6284.218232	25.857716
178.077876	6288.700837	25.862733
178.069046	6288.881980	25.867751
178.146041	6296.797468	25.872768
178.473770	6301.246552	25.877786
178.261819	6319.596558	25.882804
178.465226	6316.212911	25.887821
178.615175	6329.012452	25.892839
178.752424	6350.198193	25.897856
179.455580	6349.199311	25.902874
179.722399	6348.397743	25.907892
180.054781	6351.390710	25.912909
180.359080	6357.659736	25.917927
180.271386	6349.297347	25.922944
180.764872	6344.307233	25.927962
180.462095	6340.146444	25.932980
180.527995	6347.950385	25.937997
180.735264	6365.699591	25.943015
181.126264	6377.740323	25.948032
181.203607	6369.005713	25.953050
180.820398	6381.822514	25.958068
181.125961	6403.580620	25.963085
181.619933	6398.815644	25.968103
181.704049	6425.317479	25.973120
182.068277	6442.964446	25.978138
182.052888	6446.857561	25.983156
181.927647	6443.498263	25.988173
182.635865	6467.895911	25.993191
182.472107	6462.230756	25.998208
183.084416	6469.748376	26.003226
183.279490	6496.720273	26.008244
183.295270	6491.861810	26.013261
183.699848	6497.707953	26.018279
183.390006	6503.125588	26.023296
183.979941	6519.962769	26.028314
183.891593	6527.595401	26.033332
183.992218	6527.009508	26.038349
184.417977	6541.636429	26.043367
184.654143	6558.873113	26.048384
184.632285	6564.903935	26.053402
184.933944	6563.532718	26.058420
184.658692	6584.387648	26.063437
185.146774	6597.663132	26.068455
185.191871	6615.915883	26.073472
185.414862	6616.398159	26.078490
185.597688	6630.960560	26.083508
185.723065	6648.271563	26.088525
186.171224	6650.997380	26.093543
186.000980	6660.581767	26.098560
186.363453	6671.321681	26.103578
186.640228	6681.157478	26.108596
186.647090	6680.711505	26.113613
186.775371	6700.808443	26.118631
186.589986	6715.770409	26.123648
186.991937	6733.591820	26.128666
187.348403	6733.640943	26.133684
187.558174	6755.435053	26.138701
187.776146	6780.131556	26.143719
187.758204	6777.193914	26.148736
188.135461	6789.809000	26.153754
188.476058	6806.241931	26.158772
188.741508	6818.873152	26.163789
188.763842	6822.444315	26.168807
189.237453	6832.120099	26.173824
189.478471	6817.909079	26.178842
189.857123	6828.255011	26.183860
190.402596	6842.087475	26.188877
190.427987	6843.103296	26.193895
190.482515	6853.137373	26.198912
190.419905	6848.269701	26.203930
190.532878	6855.643197	26.208948
190.545524	6862.400076	26.213965
191.029117	6868.771994	26.218983
191.065760	6876.049428	26.224000
191.011437	6883.691573	26.229018
191.313751	6897.469756	26.234036
191.705730	6919.881363	26.239053
191.730133	6919.360030	26.244071
191.693186	6939.630272	26.249088
192.050128	6947.276163	26.254106
192.202962	6954.606104	26.259124
191.935881	6971.844485	26.264141
192.387284	6988.678283	26.269159
192.345130	7010.612030	26.274176
192.481379	7018.004596	26.279194
193.248856	7036.985111	26.284212
193.600960	7056.595819	26.289229
193.955842	7064.813883	26.294247
194.057130	7072.493414	26.299264
194.265967	7075.759745	26.304282
194.569070	7082.444310	26.309300
194.250641	7104.993251	26.314317
194.923174	7093.812931	26.319335
194.957645	7109.171320	26.324352
195.353471	7119.062541	26.329370
195.503002	7121.023433	26.334388
195.579264	7127.825044	26.339405
196.081426	7153.343870	26.344423
195.967041	7160.502264	26.349440
195.928588	7162.138238	26.354458
196.393346	7166.579106	26.359476
196.372176	7195.193795	26.364493
196.778100	7195.217424	26.369511
196.844656	7206.987133	26.374528
196.735824	7218.344786	26.379546
196.969593	7233.493949	26.384564
197.267761	7255.647457	26.389581
197.759319	7256.209030	26.394599
197.627458	7273.558499	26.399616
198.378202	7284.559163	26.404634
198.508686	7291.753552	26.409652
198.223078	7295.377279	26.414669
198.938449	7291.960815	26.419687
199.088345	7295.929215	26.424704
199.176374	7318.912203	26.429722
199.246650	7303.813787	26.434740
199.800817	7334.536535	26.439757
200.010265	7336.408796	26.444775
199.698735	7340.506216	26.449792
199.581868	7348.228228	26.454810
200.183593	7356.710455	26.459828
200.247891	7361.365612	26.464845
200.005876	7376.851067	26.469863
200.637737	7391.245468	26.474880
200.589480	7402.624748	26.479898
201.020050	7409.708964	26.484916
200.766037	7429.318685	26.489933
201.229878	7448.580632	26.494951
201.439225	7467.851574	26.499968
201.688089	7474.511403	26.504986
202.095109	7483.431479	26.510004
202.113511	7498.710993	26.515021
202.555441	7517.646644	26.520039
202.904618	7521.286827	26.525056
203.326791	7524.176975	26.530074
203.598782	7534.596916	26.535092
203.630181	7553.657149	26.540109
203.917380	7556.204160	26.545127
203.727045	7556.924094	26.550144
204.089793	7564.434649	26.555162
204.417867	7582.648851	26.560180
204.398718	7588.244076	26.565197
204.595742	7588.511724	26.570215
204.537852	7612.409234	26.575232
204.613088	7630.992121	26.580250
205.078282	7643.269661	26.585268
205.614456	7654.981800	26.590285
205.678404	7665.919001	26.595303
205.771476	7670.571071	26.600320
206.020134	7695.434060	26.605338
206.001044	7700.300784	26.610356
206.062736	7717.690431	26.615373
206.585599	7730.575203	26.620391
206.887881	7740.934357	26.625408
207.495544	7753.392432	26.630426
207.918296	7754.145757	26.635444
207.900989	7761.101719	26.640461
208.028260	7765.671769	26.645479
208.320894	7769.415865	26.650496
208.709812	7774.493222	26.655514
209.023155	7780.232842	26.660532
208.922495	7787.181323	26.665549
209.152723	7781.535655	26.670567
209.416586	7794.067108	26.675584
209.241621	7817.635362	26.680602
209.384840	7824.070999	26.685620
209.291296	7832.051666	26.690637
209.357685	7841.687457	26.695655
209.883839	7860.619056	26.700672
209.734673	7887.569874	26.705690
210.362127	7893.849133	26.710708
210.389013	7892.604330	26.715725
210.986089	7914.258863	26.720743
211.596358	7932.850579	26.725760
211.524270	7938.498782	26.730778
211.685443	7940.247561	26.735796
212.077608	7955.426380	26.740813
212.032090	7958.340326	26.745831
212.435737	7963.947739	26.750848
212.478460	7978.146240	26.755866
212.968307	7976.738299	26.760884
212.746606	8002.612814	26.765901
212.852037	8003.074392	26.770919
213.335739	8018.162536	26.775936
213.355339	8030.832988	26.780954
213.633858	8022.924304	26.785972
213.959445	8048.131142	26.790989
213.856119	8061.507946	26.796007
214.055084	8063.482843	26.801024
214.056660	8087.334226	26.806042
214.262178	8088.800815	26.811060
213.969401	8113.305766	26.816077
214.326893	8135.200244	26.821095
215.051491	8151.440388	26.826112
215.413559	8164.170143	26.831130
215.572618	8183.337636	26.836148
215.784969	8194.734286	26.841165
216.311606	8205.939605	26.846183
216.657297	8220.492318	26.851200
216.663399	8224.393347	26.856218
217.131487	8228.347215	26.861236
217.379828	8239.985266	26.866253
217.405286	8246.494879	26.871271
217.822574	8250.613885	26.876288
217.666195	8246.808821	26.881306
217.917732	8267.178024	26.886324
218.034240	8275.133659	26.891341
218.300900	8288.559004	26.896359
218.514779	8304.352038	26.901376
218.763009	8319.673922	26.906394
219.125362	8333.101609	26.911412
219.220749	8337.291940	26.916429
219.517063	8355.769839	26.921447
219.684183	8379.338328	26.926464
219.731539	8388.278176	26.931482
220.131343	8391.910985	26.936500
220.237385	8410.936288	26.941517
220.238218	8432.880657	26.946535
220.772215	8431.678834	26.951552
220.867156	8454.748971	26.956570
221.268543	8466.367416	26.961588
221.623612	8454.113851	26.966605
221.669352	8477.638743	26.971623
222.146804	8489.940911	26.976640
222.262225	8496.993413	26.981658
222.994733	8514.394396	26.986676
222.776902	8529.915573	26.991693
222.957505	8517.092177	26.996711
223.213586	8537.935138	27.001728
223.295185	8550.884040	27.006746
223.672073	8543.741764	27.011764
223.647846	8574.114322	27.016781
223.966189	8590.366120	27.021799
223.989164	8599.202208	27.026816
224.022216	8618.478476	27.031834
224.603734	8624.816817	27.036852
224.523383	8649.683683	27.041869
224.688185	8658.568047	27.046887
225.262424	8675.299863	27.051904
225.285664	8686.928964	27.056922
225.634453	8712.306310	27.061940
225.825637	8722.578920	27.066957
226.039038	8730.967737	27.071975
226.588050	8750.158129	27.076992
226.592859	8756.657973	27.082010
226.796183	8760.194944	27.087028
226.796896	8778.648925	27.092045
227.133224	8808.859965	27.097063
227.909424	8796.185261	27.102080
227.608116	8817.132498	27.107098
227.882260	8835.371234	27.112116
228.148441	8842.521855	27.117133
228.182021	8862.756914	27.122151
228.566257	8866.854763	27.127168
228.409731	8879.064281	27.132186
228.685642	8896.544278	27.137204
229.101532	8895.958985	27.142221
229.099877	8934.608401	27.147239
229.491887	8937.949615	27.152256
229.563405	8959.788513	27.157274
229.892408	8973.480609	27.162292
230.237798	8983.104866	27.167309
230.327621	9001.961846	27.172327
230.723367	9017.532565	27.177344
231.275459	9038.150050	27.182362
231.325780	9045.796427	27.187380
231.564308	9068.663357	27.192397
231.670309	9082.493214	27.197415
231.923159	9088.930156	27.202432
231.923373	9105.107442	27.207450
232.097671	9135.545943	27.212468
232.571103	9142.167011	27.217485
232.460421	9169.869025	27.222503
233.122617	9169.472241	27.227520
233.588949	9192.604965	27.232538
233.932501	9191.291199	27.237556
234.052802	9195.753327	27.242573
234.293916	9224.130637	27.247591
234.791510	9221.780039	27.252608
235.071342	9244.353683	27.257626
235.118387	9253.453180	27.262644
235.226342	9262.090491	27.267661
235.538230	9270.750038	27.272679
236.240229	9272.665606	27.277696
236.034975	9277.888883	27.282714
235.877429	9278.219085	27.287732
236.695988	9303.630823	27.292749
236.348607	9319.945314	27.297767
236.585914	9326.148617	27.302784
237.157420	9346.765660	27.307802
237.073878	9363.684080	27.312820
237.405286	9375.351776	27.317837
237.639851	9401.043691	27.322855
237.792399	9409.510663	27.327872
237.938021	9426.554337	27.332890
237.817402	9447.907351	27.337908
238.503764	9467.780114	27.342925
238.968948	9480.378890	27.347943
239.533639	9513.411279	27.352960
239.505862	9524.088438	27.357978
239.338854	9530.924974	27.362996
240.037511	9540.803917	27.368013
239.525047	9562.730676	27.373031
239.834072	9577.337957	27.378048
239.970129	9603.128393	27.383066
240.665811	9634.446632	27.388084
240.996339	9653.208687	27.393101
240.902705	9665.773120	27.398119
241.740578	9669.146377	27.403136
242.071226	9688.049452	27.408154
242.025366	9700.572936	27.413172
242.164554	9705.971027	27.418189
242.590462	9728.586602	27.423207
242.787221	9742.740750	27.428224
243.088014	9761.205368	27.433242
242.962451	9777.746769	27.438260
243.465131	9790.568031	27.443277
243.555541	9803.596843	27.448295
243.986266	9811.254781	27.453312
244.019137	9834.807437	27.458330
243.705940	9846.736374	27.463348
244.120528	9868.462332	27.468365
244.765576	9897.152991	27.473383
245.232912	9910.510319	27.478400
245.473732	9905.182752	27.483418
245.549800	9933.555512	27.488436
245.998313	9930.400004	27.493453
245.887447	9956.291674	27.498471
246.090604	9968.423692	27.503488
246.611338	9974.505588	27.508506
246.664638	10011.344669	27.513524
246.585745	10019.136533	27.518541
246.903239	10041.056794	27.523559
246.889166	10063.549398	27.528576
247.439537	10086.378870	27.533594
247.750101	10103.149459	27.538612
248.038490	10113.911838	27.543629
248.069254	10139.699270	27.548647
248.857237	10159.946820	27.553664
249.070205	10155.302002	27.558682
249.772496	10176.825666	27.563700
250.189025	10189.405474	27.568717
249.648444	10194.157463	27.573735
250.133104	10222.972888	27.578752
250.716877	10236.414444	27.583770
250.542626	10234.084906	27.588788
251.302872	10264.273570	27.593805
251.421718	10267.924879	27.598823
251.597811	10281.304643	27.603840
251.805260	10306.428242	27.608858
251.421980	10307.453515	27.613876
251.345699	10318.470853	27.618893
251.879778	10349.558824	27.623911
252.580505	10361.491561	27.628928
252.994778	10388.043150	27.633946
252.930867	10408.267131	27.638964
253.595355	10412.346653	27.643981
253.690231	10438.264191	27.648999
254.031362	10453.618473	27.654016
254.474036	10451.998345	27.659034
254.925818	10471.076119	27.664052
255.268569	10474.716478	27.669069
255.256606	10482.513264	27.674087
255.467887	10505.033063	27.679104
255.665819	10510.246055	27.684122
255.564930	10521.173069	27.689140
256.199968	10529.801182	27.694157
256.207392	10555.977559	27.699175
256.433485	10567.716311	27.704192
256.941791	10580.060697	27.709210
257.266993	10605.985354	27.714228
257.697495	10607.486695	27.719245
257.869551	10612.778044	27.724263
257.805330	10619.894254	27.729280
258.170078	10630.304060	27.734298
258.255436	10666.494977	27.739316
258.502827	10666.571605	27.744333
258.547977	10690.691460	27.749351
258.693034	10698.399389	27.754368
259.245741	10723.819513	27.759386
259.395331	10748.619360	27.764404
259.632751	10773.388979	27.769421
260.159141	10789.494429	27.774439
260.282182	10815.389806	27.779456
260.236726	10829.529794	27.784474
260.286163	10839.649158	27.789492
260.544688	10862.471243	27.794509
260.916476	10886.661104	27.799527
261.215288	10902.749912	27.804544
261.902818	10922.599883	27.809562
262.082915	10947.818813	27.814580
262.354287	10942.875010	27.819597
262.683772	10973.507224	27.824615
262.929371	10981.261699	27.829632
263.235174	10989.318186	27.834650
263.370631	11014.932966	27.839668
263.728952	11034.620043	27.844685
264.171378	11033.573394	27.849703
264.156236	11049.221080	27.854720
264.575928	11063.293876	27.859738
264.785224	11087.403751	27.864756
264.723201	11105.080653	27.869773
265.133542	11119.908152	27.874791
265.142005	11143.874833	27.879808
265.915964	11147.159718	27.884826
265.978652	11163.079829	27.889844
266.329186	11186.908917	27.894861
266.727745	11201.224810	27.899879
266.670962	11222.782344	27.904896
267.063135	11229.045884	27.909914
267.328885	11254.036082	27.914932
267.308663	11264.920338	27.919949
267.921481	11296.262625	27.924967
267.880830	11323.246219	27.929984
268.462493	11332.474424	27.935002
268.488523	11348.034456	27.940020
268.741843	11365.506715	27.945037
269.140419	11380.764166	27.950055
269.415915	11400.736376	27.955072
269.420011	11420.138191	27.960090
269.696942	11446.403054	27.965108
270.351025	11465.391873	27.970125
270.558060	11496.771658	27.975143
270.345223	11516.136953	27.980160
270.801893	11536.502442	27.985178
271.241687	11565.027551	27.990196
271.573106	11578.063681	27.995213
271.880948	11599.507907	28.000231
272.001660	11622.717018	28.005248
272.508702	11631.299916	28.010266
272.633417	11667.612635	28.015284
272.817136	11682.571058	28.020301
273.327792	11705.969534	28.025319
273.454388	11739.272710	28.030336
273.932446	11742.100054	28.035354
274.096418	11765.098182	28.040372
274.393529	11786.356933	28.045389
274.821400	11807.885598	28.050407
275.077388	11821.489003	28.055424
275.158808	11837.147499	28.060442
275.456476	11860.439585	28.065460
275.418021	11877.545432	28.070477
276.084059	11907.367530	28.075495
276.044855	11926.246912	28.080512
276.708235	11931.827795	28.085530
276.666222	11964.866228	28.090548
276.988735	11984.224781	28.095565
277.574016	12003.354807	28.100583
277.606192	12022.703864	28.105600
278.186234	12035.717410	28.110618
278.365947	12056.915559	28.115636
278.566544	12086.406010	28.120653
278.902889	12091.521809	28.125671
279.230518	12117.829814	28.130688
279.395002	12137.345439	28.135706
279.794018	12153.732501	28.140724
280.014593	12180.271795	28.145741
280.497559	12174.733305	28.150759
280.627422	12188.401190	28.155776
281.044826	12205.208329	28.160794
281.254932	12212.468997	28.165812
281.431365	12246.947513	28.170829
281.687175	12243.746194	28.175847
281.751713	12261.186803	28.180864
282.425512	12265.552042	28.185882
282.658328	12286.168181	28.190900
282.629799	12302.610277	28.195917
283.079567	12325.339032	28.200935
283.463042	12343.243065	28.205952
283.698025	12358.024264	28.210970
284.221252	12380.956039	28.215988
284.179383	12384.383067	28.221005
284.647895	12401.561703	28.226023
284.618699	12419.971249	28.231040
285.125817	12432.332234	28.236058
285.322863	12464.181167	28.241076
285.323147	12483.452535	28.246093
285.459274	12497.537989	28.251111
285.470698	12523.412804	28.256128
286.018444	12558.245831	28.261146
286.229669	12584.907876	28.266164
286.530952	12615.374555	28.271181
286.893311	12633.176829	28.276199
287.089206	12667.252015	28.281216
287.488312	12682.256143	28.286234
287.953199	12706.219859	28.291252
288.418542	12733.807645	28.296269
288.974426	12751.533957	28.301287
288.924221	12777.013616	28.306304
289.916707	12791.229653	28.311322
289.903797	12809.084667	28.316340
289.869666	12824.428375	28.321357
290.456525	12833.889797	28.326375
290.326810	12865.297947	28.331392
291.155076	12884.407000	28.336410
291.321188	12897.800050	28.341428
291.430595	12911.323810	28.346445
292.542577	12922.151338	28.351463
292.442286	12958.179541	28.356480
292.852413	12954.587021	28.361498
292.792700	12970.667805	28.366516
293.039115	12989.874689	28.371533
293.406814	12996.572353	28.376551
293.395922	13020.796351	28.381568
293.924286	13033.756218	28.386586
294.159772	13049.555101	28.391604
294.275418	13082.703711	28.396621
294.893657	13101.995842	28.401639
294.685321	13123.282352	28.406656
295.277089	13142.585208	28.411674
295.441226	13167.124019	28.416692
295.396365	13185.463752	28.421709
295.906968	13202.659138	28.426727
295.993317	13245.692850	28.431744
296.206625	13267.462976	28.436762
296.790445	13288.272163	28.441780
297.179939	13321.229473	28.446797
297.450748	13349.176633	28.451815
297.585640	13372.819253	28.456832
297.790695	13392.079145	28.461850
298.333400	13414.964266	28.466868
298.377001	13441.292992	28.471885
298.994957	13449.055690	28.476903
299.385826	13483.453357	28.481920
299.688862	13502.995015	28.486938
300.486752	13514.840790	28.491956
300.111930	13531.316133	28.496973
300.316974	13551.556351	28.501991
300.483580	13573.801036	28.507008
300.686889	13596.031808	28.512026
301.373118	13610.596995	28.517044
301.463047	13640.703428	28.522061
301.854742	13651.970339	28.527079
301.882920	13682.339177	28.532096
302.357597	13700.480202	28.537114
302.755204	13713.017845	28.542132
302.799719	13742.758507	28.547149
303.408542	13765.182522	28.552167
303.797940	13780.257037	28.557184
304.198911	13803.040060	28.562202
304.310848	13829.039813	28.567220
304.262933	13845.773475	28.572237
304.989169	13876.432332	28.577255
305.230926	13901.926980	28.582272
305.496392	13918.498636	28.587290
305.973595	13940.656266	28.592308
306.092283	13968.251430	28.597325
306.574406	13990.627355	28.602343
306.534851	14023.770439	28.607360
307.146367	14051.561669	28.612378
307.504054	14064.689236	28.617396
307.668497	14090.543637	28.622413
308.266305	14104.600703	28.627431
308.257994	14137.215679	28.632448
308.290771	14166.691164	28.637466
308.946572	14186.187973	28.642484
308.896683	14210.543105	28.647501
309.283196	14238.636571	28.652519
309.515024	14270.878062	28.657536
309.865213	14295.854295	28.662554
310.357328	14334.581665	28.667572
310.678243	14354.546878	28.672589
311.277739	14380.123426	28.677607
311.344275	14405.740790	28.682624
311.468875	14433.014291	28.687642
312.158856	14458.100102	28.692660
312.241535	14502.078543	28.697677
312.767328	14507.044049	28.702695
313.393766	14527.920282	28.707712
313.410955	14556.890041	28.712730
314.048449	14561.977364	28.717748
314.312864	14591.667490	28.722765
314.154485	14621.745848	28.727783
314.489122	14641.063034	28.732800
314.910464	14658.427578	28.737818
315.264112	14683.613429	28.742836
315.064242	14709.929278	28.747853
315.675263	14739.798795	28.752871
316.286110	14765.460750	28.757888
316.464148	14791.022478	28.762906
317.180186	14809.575578	28.767924
317.103036	14830.335206	28.772941
317.916651	14851.237664	28.777959
318.248583	14873.866551	28.782976
318.402416	14893.445566	28.787994
319.082140	14909.990769	28.793012
319.031700	14934.539335	28.798029
319.437270	14964.953805	28.803047
319.742592	14978.213686	28.808064
319.718421	15000.189266	28.813082
320.034376	15016.033505	28.818100
320.319618	15052.850501	28.823117
320.543215	15077.935526	28.828135
320.921870	15090.015621	28.833152
320.932877	15118.927515	28.838170
321.796176	15143.511398	28.843188
321.993023	15165.029911	28.848205
321.994162	15196.430399	28.853223
322.411023	15197.125988	28.858240
322.546809	15234.467658	28.863258
323.174370	15245.870067	28.868276
322.791022	15285.414111	28.873293
323.265014	15309.958550	28.878311
323.880176	15341.590401	28.883328
323.796924	15364.721949	28.888346
324.243570	15395.871136	28.893364
324.904008	15441.835349	28.898381
325.167669	15468.383152	28.903399
325.384091	15493.325013	28.908416
325.275911	15522.427515	28.913434
326.093562	15548.143219	28.918452
326.335736	15589.831993	28.923469
326.635077	15613.932951	28.928487
327.199128	15648.405876	28.933504
327.357045	15682.422743	28.938522
327.874489	15701.870161	28.943540
327.989019	15740.746783	28.948557
328.473048	15768.483212	28.953575
328.880527	15785.015973	28.958592
329.426409	15817.788606	28.963610
329.640017	15838.053894	28.968628
330.111471	15863.278842	28.973645
330.728481	15892.629404	28.978663
330.837829	15925.620941	28.983680
331.053019	15943.651318	28.988698
331.473542	15960.245142	28.993716
331.956045	15999.736120	28.998733
331.881835	16012.838903	29.003751
332.393958	16046.282651	29.008768
332.504400	16079.695115	29.013786
333.052425	16098.691940	29.018804
333.631718	16137.109746	29.023821
333.741552	16152.749587	29.028839
334.483218	16167.103035	29.033856
334.952497	16204.114442	29.038874
335.253989	16215.232554	29.043892
335.644287	16233.056229	29.048909
335.905339	16252.877631	29.053927
336.583125	16252.176344	29.058944
336.464109	16269.406504	29.063962
337.281213	16290.921744	29.068980
337.621932	16306.690649	29.073997
337.792814	16332.424607	29.079015
338.106161	16340.131854	29.084032
338.081721	16358.837426	29.089050
338.609152	16372.473097	29.094068
338.808084	16408.282971	29.099085
338.746382	16420.644843	29.104103
339.705846	16443.805810	29.109120
339.462190	16482.891517	29.114138
339.776301	16488.645967	29.119156
340.633859	16530.230744	29.124173
340.453097	16541.455542	29.129191
341.036972	16565.781981	29.134208
341.235843	16598.812093	29.139226
341.311371	16622.812818	29.144244
341.884125	16651.688201	29.149261
342.318104	16681.973513	29.154279
342.848569	16708.770826	29.159296
342.852797	16737.732404	29.164314
343.312829	16758.749317	29.169332
343.230392	16782.870938	29.174349
343.745578	16811.091002	29.179367
344.047319	16840.714428	29.184384
344.178816	16877.554625	29.189402
344.435532	16897.256163	29.194420
344.483850	16919.020599	29.199437
344.902381	16958.340053	29.204455
345.264107	16992.642766	29.209472
345.272750	17029.776267	29.214490
345.813756	17053.402836	29.219508
346.274216	17090.244327	29.224525
346.991607	17124.204855	29.229543
347.720650	17159.373994	29.234560
347.670848	17194.451219	29.239578
347.870038	17228.770243	29.244596
348.233931	17252.609191	29.249613
348.615906	17289.322242	29.254631
349.198898	17315.670550	29.259648
349.531135	17336.818070	29.264666
350.174587	17368.567380	29.269684
350.476539	17399.968097	29.274701
350.917666	17428.247165	29.279719
351.349270	17455.457645	29.284736
351.552658	17487.418587	29.289754
351.980976	17508.102825	29.294772
352.286558	17537.203586	29.299789
352.565376	17558.755834	29.304807
352.961737	17580.239830	29.309824
353.111169	17610.854420	29.314842
353.487896	17639.557447	29.319860
353.472671	17682.173564	29.324877
353.924237	17712.068553	29.329895
354.305232	17740.859317	29.334912
354.258635	17785.463722	29.339930
354.920940	17821.119735	29.344948
355.442850	17861.421996	29.349965
356.069263	17894.893189	29.354983
356.639294	17915.828787	29.360000
356.782945	17949.934668	29.365018
357.505491	17969.443894	29.370036
358.150685	17997.962911	29.375053
358.232158	18034.386806	29.380071
359.267306	18031.747578	29.385088
359.410529	18054.199248	29.390106
359.491860	18085.243665	29.395124
359.848185	18089.104976	29.400141
359.922605	18118.796628	29.405159
360.517621	18147.125591	29.410176
360.620534	18168.165475	29.415194
360.824190	18191.748534	29.420212
361.344251	18224.813962	29.425229
361.579181	18260.945046	29.430247
362.004227	18284.231584	29.435264
362.435126	18323.902179	29.440282
362.783495	18357.727612	29.445300
362.844610	18371.779301	29.450317
363.202287	18417.075219	29.455335
363.524595	18437.008929	29.460352
363.476517	18484.175291	29.465370
364.077029	18516.502936	29.470388
364.326732	18549.755541	29.475405
364.628529	18604.607036	29.480423
365.334632	18620.634630	29.485440
365.819521	18658.906842	29.490458
365.949576	18693.809367	29.495476
366.722547	18717.690039	29.500493
366.760312	18748.104505	29.505511
367.451106	18777.433850	29.510528
368.029074	18794.874639	29.515546
368.363931	18814.351185	29.520564
369.102554	18835.312118	29.525581
369.160463	18851.828481	29.530599
369.407056	18873.663620	29.535616
369.791925	18910.865298	29.540634
369.725678	18936.492748	29.545652
370.245467	18961.544229	29.550669
370.235281	18989.336216	29.555687
370.795830	19024.713719	29.560704
370.908076	19059.753942	29.565722
370.919542	19096.614189	29.570740
371.856563	19126.418931	29.575757
371.980987	19174.654297	29.580775
372.435714	19206.074193	29.585792
372.999153	19241.401239	29.590810
373.114710	19278.619859	29.595828
373.363407	19310.062954	29.600845
373.886884	19359.434098	29.605863
373.904241	19387.368799	29.610880
374.105917	19429.641462	29.615898
374.453065	19478.304360	29.620916
375.232986	19515.531983	29.625933
375.577981	19563.623271	29.630951
375.859706	19606.726510	29.635968
376.358450	19643.874763	29.640986
376.824138	19683.322174	29.646004
377.757498	19713.929375	29.651021
377.953343	19750.820513	29.656039
378.574381	19774.029479	29.661056
379.036107	19811.017125	29.666074
379.635466	19836.389400	29.671092
380.107625	19858.213793	29.676109
380.091501	19892.764653	29.681127
380.542523	19925.518570	29.686144
381.158799	19945.567900	29.691162
381.232172	19986.773888	29.696180
381.771654	20011.773258	29.701197
381.941152	20046.074651	29.706215
382.522600	20077.503638	29.711232
382.538676	20110.419627	29.716250
383.234976	20139.501402	29.721268
383.818207	20175.427779	29.726285
384.042234	20202.399622	29.731303
384.477836	20233.118386	29.736320
384.933214	20265.843878	29.741338
384.948491	20297.734117	29.746356
385.469069	20321.345092	29.751373
385.668423	20365.403455	29.756391
386.075195	20395.375323	29.761408
386.516501	20433.925245	29.766426
386.961387	20452.825901	29.771444
387.738925	20484.007290	29.776461
388.135728	20519.660954	29.781479
388.337965	20542.252848	29.786496
388.576920	20574.587482	29.791514
389.075262	20601.057482	29.796532
389.481723	20636.309381	29.801549
390.086621	20678.444507	29.806567
390.151490	20704.090850	29.811584
390.362937	20730.154427	29.816602
390.682861	20768.971104	29.821620
391.020036	20796.995639	29.826637
391.632048	20828.681113	29.831655
391.883416	20866.833034	29.836672
392.305137	20913.342215	29.841690
392.436288	20949.177836	29.846708
393.737691	20976.639803	29.851725
393.867036	21004.185084	29.856743
394.011516	21011.674907	29.861760
394.716684	21042.580799	29.866778
394.948483	21075.223424	29.871796
395.428425	21093.635032	29.876813
395.474116	21129.001170	29.881831
395.860238	21162.324745	29.886848
396.221524	21186.604900	29.891866
396.504648	21229.723138	29.896884
396.859816	21257.999292	29.901901
397.113897	21290.935042	29.906919
397.501504	21333.684724	29.911936
397.686366	21375.427500	29.916954
397.504461	21423.302190	29.921972
398.435820	21459.520660	29.926989
398.549624	21509.818754	29.932007
399.045629	21553.785521	29.937024
399.453063	21593.516661	29.942042
399.720342	21644.029439	29.947060
400.224452	21693.623526	29.952077
400.659771	21742.904353	29.957095
401.259487	21777.131920	29.962112
401.930086	21823.697109	29.967130
402.252922	21875.082707	29.972148
403.058010	21901.081571	29.977165
403.130707	21943.170639	29.982183
403.554662	21986.981750	29.987200
404.258064	22014.873725	29.992218
404.336601	22072.734337	29.997236
404.844916	22101.595181	30.002253
405.260900	22149.016857	30.007271
405.518254	22191.883262	30.012288
406.443631	22218.693619	30.017306
406.580974	22261.312003	30.022324
406.973260	22291.575028	30.027341
407.445258	22333.908127	30.032359
407.621645	22362.453746	30.037376
408.667495	22408.335804	30.042394
409.188758	22444.934747	30.047412
409.526618	22474.860235	30.052429
409.738839	22506.987014	30.057447
409.976553	22551.325424	30.062464
410.756923	22575.826885	30.067482
411.231917	22627.866025	30.072500
411.706616	22644.864380	30.077517
411.752337	22683.871107	30.082535
411.971352	22724.413337	30.087552
412.287464	22754.686625	30.092570
412.643980	22799.518476	30.097588
413.075424	22839.057820	30.102605
413.479013	22878.436308	30.107623
413.842372	22921.058440	30.112640
414.356966	22954.999749	30.117658
414.637541	23002.991730	30.122676
415.378818	23048.391355	30.127693
415.889482	23091.970283	30.132711
415.996866	23128.519254	30.137728
416.422275	23169.860952	30.142746
417.022231	23212.447890	30.147764
417.024247	23248.773292	30.152781
417.699952	23286.904758	30.157799
418.083811	23328.698339	30.162816
418.813950	23370.214081	30.167834
418.741036	23424.944616	30.172852
419.471336	23446.396783	30.177869
419.265053	23493.125639	30.182887
419.960110	23546.075716	30.187904
420.103573	23579.444168	30.192922
420.856366	23635.412316	30.197940
420.824416	23677.956600	30.202957
421.186066	23712.164362	30.207975
421.648035	23765.122095	30.212992
422.590206	23807.876324	30.218010
422.845723	23853.091886	30.223028
423.112767	23893.632139	30.228045
423.674198	23941.709683	30.233063
423.904938	23974.105820	30.238080
424.485759	24011.515090	30.243098
424.882209	24075.186181	30.248116
425.103546	24103.287395	30.253133
425.875106	24146.045435	30.258151
426.105267	24203.306460	30.263168
426.411593	24235.979164	30.268186
427.347040	24281.290108	30.273204
427.853453	24337.126251	30.278221
428.576330	24360.775720	30.283239
428.644143	24410.128199	30.288256
429.253128	24440.865436	30.293274
429.958257	24472.067776	30.298292
430.329080	24507.437742	30.303309
431.218346	24536.416427	30.308327
431.333718	24586.141575	30.313344
431.874367	24606.432890	30.318362
432.172923	24636.026525	30.323380
432.431828	24677.572861	30.328397
432.811103	24707.820289	30.333415
433.114385	24765.432226	30.338432
433.367728	24802.455823	30.343450
433.522905	24842.239436	30.348468
434.134122	24887.050509	30.353485
434.391352	24937.054428	30.358503
434.573508	24992.883217	30.363520
435.104962	25037.196957	30.368538
435.320712	25095.210802	30.373556
436.031600	25154.503899	30.378573
436.294538	25207.856962	30.383591
437.022395	25258.074226	30.388608
437.590920	25310.189732	30.393626
437.403115	25354.315619	30.398644
437.896288	25419.230974	30.403661
438.512019	25463.304827	30.408679
438.933294	25525.874988	30.413696
439.684159	25566.834459	30.418714
440.245379	25615.803002	30.423732
440.654133	25665.692566	30.428749
440.937528	25717.004876	30.433767
441.416079	25768.755028	30.438784
442.320567	25810.900796	30.443802
442.903129	25862.244547	30.448820
443.630461	25901.311646	30.453837
444.380456	25936.587252	30.458855
444.079441	25985.617287	30.463872
444.697683	26008.655555	30.468890
445.148925	26058.627558	30.473908
445.451240	26094.557766	30.478925
445.991370	26135.056669	30.483943
446.179284	26191.777836	30.488960
446.936378	26224.791484	30.493978
447.567993	26271.075724	30.498996
447.991587	26319.618003	30.504013
448.288192	26348.059001	30.509031
448.588653	26414.949669	30.514048
448.902436	26447.585957	30.519066
449.639431	26482.448512	30.524084
449.923959	26521.195924	30.529101
450.266500	26572.307057	30.534119
450.734797	26600.461483	30.539136
451.398721	26643.549520	30.544154
451.652572	26680.491945	30.549172
451.764464	26720.646641	30.554189
452.614119	26751.296252	30.559207
452.969327	26794.416741	30.564224
453.538153	26834.332212	30.569242
453.939831	26875.969125	30.574260
454.394730	26912.926152	30.579277
454.962762	26948.934113	30.584295
455.216764	27004.205632	30.589312
455.576517	27037.251790	30.594330
456.052321	27090.834197	30.599348
456.129771	27122.574037	30.604365
456.825997	27159.611587	30.609383
457.293455	27215.450963	30.614400
457.857827	27257.181783	30.619418
458.420193	27303.234227	30.624436
458.693713	27353.728257	30.629453
459.381092	27394.912347	30.634471
459.694768	27447.093807	30.639488
460.226900	27493.388318	30.644506
460.513731	27538.912846	30.649524
460.977387	27592.214944	30.654541
461.575132	27628.976434	30.659559
461.884271	27679.083874	30.664576
462.532794	27721.590477	30.669594
462.998459	27772.978186	30.674612
463.220897	27828.279644	30.679629
464.126961	27868.384689	30.684647
464.215736	27916.554655	30.689664
464.536604	27973.048402	30.694682
464.876600	28034.942469	30.699700
465.546870	28074.903996	30.704717
466.036264	28128.572554	30.709735
466.416954	28188.624644	30.714752
466.872507	28239.359315	30.719770
467.634633	28288.885853	30.724788
467.939232	28351.808907	30.729805
468.359272	28398.944496	30.734823
468.984677	28457.969786	30.739840
469.052325	28504.731726	30.744858
469.450746	28549.445584	30.749876
470.306012	28610.597332	30.754893
470.655586	28669.675217	30.759911
470.908853	28730.740720	30.764928
471.560864	28766.741767	30.769946
472.615327	28829.318727	30.774964
472.829494	28890.779250	30.779981
474.102556	28929.860883	30.784999
474.589385	28972.905145	30.790016
474.792777	29009.113289	30.795034
475.232910	29042.307737	30.800052
475.346454	29089.905918	30.805069
476.537365	29134.660724	30.810087
476.586979	29160.614112	30.815104
477.011302	29222.567897	30.820122
477.477681	29261.745679	30.825140
477.679254	29315.910251	30.830157
478.257793	29363.795144	30.835175
478.634867	29406.183543	30.840192
479.085614	29467.774221	30.845210
479.429728	29514.843371	30.850228
479.836146	29558.038015	30.855245
480.270429	29614.830687	30.860263
480.442344	29681.950834	30.865280
480.830492	29729.000673	30.870298
481.153832	29794.597809	30.875316
481.715336	29847.202988	30.880333
482.372248	29895.997551	30.885351
482.894884	29955.199493	30.890368
483.342080	30011.953472	30.895386
484.252850	30057.898921	30.900404
484.425325	30112.982477	30.905421
484.781474	30152.391838	30.910439
485.550853	30214.891550	30.915456
485.778309	30258.007079	30.920474
486.800711	30310.449196	30.925492
487.759222	30365.498351	30.930509
487.316720	30396.878953	30.935527
488.197663	30446.625482	30.940544
488.351778	30502.984656	30.945562
488.961533	30547.618276	30.950580
489.404151	30609.097609	30.955597
489.856193	30655.498981	30.960615
489.979664	30710.627220	30.965632
490.755869	30780.418515	30.970650
491.293260	30830.263899	30.975668
491.816731	30886.648480	30.980685
492.125616	30952.593078	30.985703
492.582081	30996.464463	30.990720
493.040004	31068.997396	30.995738
493.787076	31118.174843	31.000756
493.958367	31181.467722	31.005773
494.710489	31239.475127	31.010791
495.128652	31304.283022	31.015808
495.315917	31366.409779	31.020826
496.186226	31417.940192	31.025844
496.896024	31496.903996	31.030861
497.467520	31539.256001	31.035879
498.191914	31592.114013	31.040896
498.393660	31650.699552	31.045914
499.113001	31700.823392	31.050932
499.560180	31767.754645	31.055949
500.170752	31799.859816	31.060967
500.812098	31866.279817	31.065984
500.956319	31928.854219	31.071002
502.107122	31966.849173	31.076020
502.398684	32017.644029	31.081037
502.985096	32083.013842	31.086055
503.514094	32132.204920	31.091072
504.031391	32175.933543	31.096090
504.736068	32219.041331	31.101108
504.889250	32269.806138	31.106125
505.454195	32312.848896	31.111143
505.905357	32368.814791	31.116160
506.144739	32418.221727	31.121178
506.844128	32467.117415	31.126196
506.973832	32543.380027	31.131213
507.358937	32594.344093	31.136231
507.960678	32646.114940	31.141248
508.554859	32707.582906	31.146266
509.187385	32760.065218	31.151284
509.645296	32810.781249	31.156301
510.200669	32866.274014	31.161319
510.852859	32929.765098	31.166336
511.184278	32986.421631	31.171354
512.198679	33031.240842	31.176372
512.513130	33085.458379	31.181389
513.048323	33141.308726	31.186407
513.354041	33179.966509	31.191424
513.640604	33253.407602	31.196442
514.266833	33300.105872	31.201460
514.622759	33353.396051	31.206477
515.424221	33412.462645	31.211495
515.939867	33468.191045	31.216512
516.533687	33522.575181	31.221530
516.756720	33563.187955	31.226548
517.406071	33613.423465	31.231565
518.294917	33658.331272	31.236583
518.433148	33712.254843	31.241600
518.618434	33757.752411	31.246618
519.373356	33791.380327	31.251636
520.066836	33867.075918	31.256653
519.908515	33922.557364	31.261671
520.641807	33975.209654	31.266688
520.990367	34042.244714	31.271706
521.591744	34102.965369	31.276724
522.143010	34155.948025	31.281741
522.673802	34206.040720	31.286759
523.418000	34270.344979	31.291776
523.553790	34330.695250	31.296794
524.472111	34387.947209	31.301812
524.648650	34449.748962	31.306829
525.233695	34517.639746	31.311847
525.685682	34579.484806	31.316864
526.351172	34661.638183	31.321882
526.608490	34714.797279	31.326900
527.366386	34783.973213	31.331917
527.869370	34868.707189	31.336935
528.142387	34912.962574	31.341952
528.629026	34991.909450	31.346970
529.495826	35042.479134	31.351988
529.980814	35110.814707	31.357005
530.155564	35180.618638	31.362023
531.151861	35253.212369	31.367040
531.374012	35312.633428	31.372058
532.177034	35383.546127	31.377076
532.595237	35454.213419	31.382093
533.324167	35515.485841	31.387111
533.881600	35578.067992	31.392128
533.958526	35654.349533	31.397146
534.657826	35725.968658	31.402164
535.132226	35798.534054	31.407181
535.729689	35870.230536	31.412199
536.359693	35940.142112	31.417216
536.576486	36011.693762	31.422234
537.182447	36081.082856	31.427252
538.191994	36159.427827	31.432269
538.187601	36230.291063	31.437287
538.945706	36305.317325	31.442304
539.398039	36374.540429	31.447322
540.365855	36437.420717	31.452340
540.981580	36509.157767	31.457357
541.051082	36578.135622	31.462375
542.378278	36641.301251	31.467392
543.068260	36708.217349	31.472410
543.397730	36765.539494	31.477428
543.824984	36833.742861	31.482445
544.441638	36893.694152	31.487463
544.867790	36959.250400	31.492480
545.353911	37028.347366	31.497498
545.889436	37078.270611	31.502516
546.496103	37152.886761	31.507533
547.047212	37217.284024	31.512551
547.890148	37281.926819	31.517568
548.474465	37351.217099	31.522586
549.017099	37405.586818	31.527604
549.491557	37467.412903	31.532621
550.117686	37531.284476	31.537639
550.711608	37587.154833	31.542656
551.153781	37644.625275	31.547674
551.805709	37699.817328	31.552692
552.246181	37753.949336	31.557709
552.577608	37831.378437	31.562727
553.173081	37874.833582	31.567744
553.541860	37941.753671	31.572762
553.862824	38001.438730	31.577780
554.441588	38061.737869	31.582797
554.894880	38125.100403	31.587815
555.742722	38191.973853	31.592832
556.107916	38260.975587	31.597850
556.490724	38326.332508	31.602868
557.055610	38387.512429	31.607885
557.218578	38456.661932	31.612903
558.298834	38523.119482	31.617920
558.429260	38602.693399	31.622938
559.069892	38687.848749	31.627956
559.663580	38742.687491	31.632973
560.569924	38823.210481	31.637991
561.336460	38891.712772	31.643008
561.743670	38960.280985	31.648026
562.213542	39023.037927	31.653044
563.009292	39095.453063	31.658061
563.288696	39165.813823	31.663079
563.632289	39223.889475	31.668096
564.392839	39302.923662	31.673114
565.477563	39363.165661	31.678132
565.875841	39448.004791	31.683149
566.101287	39517.400521	31.688167
566.826034	39572.450537	31.693184
567.774400	39656.417009	31.698202
568.206797	39720.135769	31.703220
568.749243	39782.097410	31.708237
569.199111	39857.754344	31.713255
569.764386	39920.656447	31.718272
570.867566	39998.437634	31.723290
571.638014	40049.248795	31.728308
572.482877	40101.572363	31.733325
572.791249	40180.558793	31.738343
573.427469	40224.805113	31.743360
573.882632	40285.738098	31.748378
574.583878	40351.327477	31.753396
575.272073	40405.328632	31.758413
575.662562	40470.325843	31.763431
576.343777	40530.269047	31.768448
577.088883	40578.870004	31.773466
577.468418	40651.028644	31.778484
578.169022	40714.094211	31.783501
578.175717	40772.492436	31.788519
578.946680	40845.461556	31.793536
579.453035	40918.155858	31.798554
579.624419	40973.317287	31.803572
580.376487	41039.077510	31.808589
580.941365	41113.047653	31.813607
581.408521	41178.890159	31.818624
581.786778	41262.285826	31.823642
582.150936	41347.679202	31.828660
583.104623	41403.243031	31.833677
583.513494	41494.191733	31.838695
584.067616	41567.673045	31.843712
584.270431	41653.959425	31.848730
585.231379	41730.707672	31.853748
585.807893	41792.676815	31.858765
586.474144	41875.841454	31.863783
586.934916	41949.623819	31.868800
587.638587	42035.794542	31.873818
588.187372	42121.707140	31.878836
588.985043	42194.936073	31.883853
589.349695	42271.128451	31.888871
589.735584	42347.153482	31.893888
590.730099	42412.626037	31.898906
591.556605	42479.957541	31.903924
592.275512	42545.157247	31.908941
592.714757	42596.686808	31.913959
593.509489	42658.881689	31.918976
594.159045	42733.463113	31.923994
594.629820	42797.887063	31.929012
595.188208	42860.645704	31.934029
595.539900	42928.009915	31.939047
595.927258	42987.428804	31.944064
596.497025	43051.199588	31.949082
596.965621	43129.979661	31.954100
598.023052	43196.385380	31.959117
598.206371	43281.514516	31.964135
598.789199	43350.635254	31.969152
599.325478	43425.149783	31.974170
600.065809	43512.682015	31.979188
600.546532	43587.029578	31.984205
600.921085	43668.911895	31.989223
601.718791	43734.506885	31.994240
602.276391	43808.902624	31.999258
602.833525	43900.012330	32.004276
603.674922	43973.850411	32.009293
603.663261	44062.153485	32.014311
604.250049	44142.433752	32.019328
605.170899	44228.588298	32.024346
605.672181	44312.946663	32.029364
606.415705	44399.690105	32.034381
606.993780	44476.702429	32.039399
607.527488	44563.639148	32.044416
608.369651	44649.161414	32.049434
608.895531	44734.521619	32.054452
609.564884	44814.102872	32.059469
610.119535	44914.459193	32.064487
610.485389	44996.756076	32.069504
611.545564	45077.391577	32.074522
612.210619	45157.742227	32.079540
612.688092	45237.394865	32.084557
613.377401	45329.503229	32.089575
613.990981	45411.666305	32.094592
614.876442	45483.340317	32.099610
615.192392	45580.601234	32.104628
616.259702	45656.558841	32.109645
616.784370	45735.154396	32.114663
617.303382	45822.001521	32.119680
617.650392	45903.585617	32.124698
618.165011	45985.729669	32.129716
619.025483	46072.092145	32.134733
619.626367	46166.483124	32.139751
620.688656	46245.291983	32.144768
621.135242	46320.082337	32.149786
621.570602	46411.082320	32.154804
622.452706	46495.112932	32.159821
623.287791	46556.426916	32.164839
623.654328	46635.819641	32.169856
624.099792	46728.650869	32.174874
624.748505	46813.195083	32.179892
625.242463	46894.986558	32.184909
626.042404	46990.043465	32.189927
626.397630	47074.097373	32.194944
626.950615	47156.587541	32.199962
627.330596	47262.687958	32.204980
628.329591	47339.828833	32.209997
628.857911	47420.000188	32.215015
629.253953	47506.256494	32.220032
630.253088	47590.247402	32.225050
630.980083	47673.885759	32.230068
632.279377	47761.108724	32.235085
633.166744	47830.855688	32.240103
633.305356	47896.555177	32.245120
634.304381	47968.425166	32.250138
634.436007	48041.029191	32.255156
634.907379	48094.655904	32.260173
635.396915	48181.597720	32.265191
636.278364	48245.931560	32.270208
637.054666	48322.942708	32.275226
637.446834	48399.575515	32.280244
638.091415	48477.821658	32.285261
638.611048	48548.475147	32.290279
638.965373	48635.864530	32.295296
639.760076	48707.268966	32.300314
640.069482	48797.404402	32.305332
640.653365	48882.464366	32.310349
641.630724	48971.865044	32.315367
641.776443	49059.309773	32.320384
643.045847	49149.373590	32.325402
643.399843	49227.512914	32.330420
643.803373	49315.292038	32.335437
644.595285	49395.927174	32.340455
645.336120	49504.169027	32.345472
645.990920	49582.992788	32.350490
646.594545	49688.608757	32.355508
647.385771	49777.030221	32.360525
647.416390	49859.087855	32.365543
647.865221	49966.461553	32.370560
648.869871	50048.204385	32.375578
649.314842	50159.833784	32.380596
650.295941	50251.977946	32.385613
651.036135	50353.229423	32.390631
651.630594	50455.152930	32.395648
652.536988	50533.866423	32.400666
653.059205	50636.226022	32.405684
653.854039	50730.920345	32.410701
655.129437	50817.175908	32.415719
655.311408	50913.440931	32.420736
655.919918	51002.747803	32.425754
656.706603	51089.319015	32.430772
657.426114	51187.372653	32.435789
657.801120	51287.530276	32.440807
658.615972	51378.671382	32.445824
659.234642	51461.251461	32.450842
660.001188	51562.991351	32.455860
660.878495	51650.304969	32.460877
661.460592	51746.362789	32.465895
662.102507	51832.648574	32.470912
662.942711	51919.517888	32.475930
663.335732	52021.223974	32.480948
663.919160	52103.591535	32.485965
664.850194	52194.717312	32.490983
665.351432	52282.977115	32.496000
666.450518	52374.562393	32.501018
666.804289	52468.823271	32.506036
667.542999	52563.160009	32.511053
668.251060	52637.811939	32.516071
669.086210	52741.356548	32.521088
669.594962	52823.376274	32.526106
670.091796	52907.445075	32.531124
670.774892	53002.488025	32.536141
671.307592	53100.752794	32.541159
671.693900	53200.337275	32.546176
672.807412	53292.069807	32.551194
673.366245	53397.988316	32.556212
673.986669	53479.284830	32.561229
674.493961	53573.633114	32.566247
675.171337	53678.333271	32.571264
676.117781	53768.314132	32.576282
676.846751	53872.514052	32.581300
677.364454	53955.585777	32.586317
678.397239	54028.780624	32.591335
678.380933	54130.559043	32.596352
679.028849	54206.263013	32.601370
680.134627	54298.266905	32.606388
680.348899	54386.482574	32.611405
680.659218	54477.456235	32.616423
681.545908	54581.962414	32.621440
682.177699	54678.595124	32.626458
682.787767	54785.567769	32.631476
683.748409	54876.688595	32.636493
684.484142	54973.261370	32.641511
684.749356	55081.827818	32.646528
685.675974	55156.459626	32.651546
686.634782	55268.482168	32.656564
686.972358	55382.395929	32.661581
688.223704	55465.795164	32.666599
688.906826	55581.422049	32.671616
689.505083	55667.899473	32.676634
690.356517	55755.118907	32.681652
691.185884	55851.920629	32.686669
692.193681	55947.101188	32.691687
692.299930	56040.636736	32.696704
692.945866	56144.413864	32.701722
693.873128	56240.405235	32.706740
694.396304	56336.255305	32.711757
695.325548	56420.128791	32.716775
696.430168	56519.030236	32.721792
696.953021	56601.771127	32.726810
697.548147	56711.296692	32.731828
698.138219	56805.103470	32.736845
698.643611	56899.095276	32.741863
699.276135	57011.383807	32.746880
699.989567	57100.704446	32.751898
700.907768	57201.523011	32.756916
701.349543	57299.349942	32.761933
702.075277	57415.050035	32.766951
702.792125	57522.436931	32.771968
702.916043	57624.772605	32.776986
703.870372	57732.538450	32.782004
704.404804	57847.103692	32.787021
705.220684	57948.442131	32.792039
705.739805	58067.156290	32.797056
706.657348	58177.192759	32.802074
707.592749	58289.008814	32.807092
707.930115	58397.076035	32.812109
709.087504	58500.408216	32.817127
709.837862	58617.457175	32.822144
710.557835	58716.003407	32.827162
711.345039	58820.801207	32.832180
711.630020	58938.421788	32.837197
712.804469	59053.747664	32.842215
713.082325	59162.309106	32.847232
713.876035	59262.394049	32.852250
714.997061	59373.642073	32.857268
715.656274	59485.965425	32.862285
716.501917	59574.656037	32.867303
716.906569	59691.806288	32.872320
718.058120	59795.759107	32.877338
718.436271	59903.897241	32.882356
719.150032	60011.759352	32.887373
720.141362	60105.104629	32.892391
720.724051	60228.175220	32.897408
721.363014	60318.843338	32.902426
722.066756	60433.098409	32.907444
722.984390	60545.391326	32.912461
723.546782	60647.657399	32.917479
723.869712	60744.181045	32.922496
724.653108	60859.822025	32.927514
725.326932	60967.373544	32.932532
725.836385	61066.250465	32.937549
726.660461	61176.173473	32.942567
727.186610	61296.371769	32.947584
727.938935	61402.092524	32.952602
728.742659	61502.825263	32.957620
729.316456	61625.166408	32.962637
730.055763	61725.158817	32.967655
730.582660	61845.846887	32.972672
731.379959	61968.829436	32.977690
732.239269	62075.231239	32.982708
732.773146	62206.500111	32.987725
733.586089	62306.919314	32.992743
734.516940	62430.211248	32.997760
734.819391	62546.111918	33.002778
735.570293	62661.736940	33.007796
736.354025	62783.532126	33.012813
737.262802	62891.598588	33.017831
738.402854	63021.540143	33.022848
739.262448	63139.747599	33.027866
740.234107	63248.842117	33.032884
740.836193	63379.013837	33.037901
741.949410	63491.183308	33.042919
742.083370	63598.559798	33.047936
743.032206	63720.314342	33.052954
743.987728	63829.225002	33.057972
744.560886	63940.613875	33.062989
745.273073	64064.191968	33.068007
745.808886	64178.666477	33.073024
746.796863	64292.415915	33.078042
747.391912	64417.273307	33.083060
748.010746	64544.384069	33.088077
748.817843	64669.005704	33.093095
749.427705	64798.666832	33.098112
750.831185	64912.660809	33.103130
752.452745	65002.561741	33.108148
753.037221	65125.851251	33.113165
753.853637	65219.893618	33.118183
754.381972	65317.871448	33.123200
755.053794	65433.152208	33.128218
755.936496	65530.914501	33.133236
756.335054	65658.277100	33.138253
757.052896	65769.689895	33.143271
757.602236	65888.248842	33.148288
758.220207	65999.913254	33.153306
759.348035	66120.419774	33.158324
759.813271	66236.971781	33.163341
760.721464	66363.603452	33.168359
761.715774	66475.758237	33.173376
762.590951	66590.107886	33.178394
762.766387	66713.025562	33.183412
763.431480	66833.353452	33.188429
764.482484	66947.916250	33.193447
765.093142	67062.052988	33.198464
765.936926	67188.270445	33.203482
766.907131	67295.022298	33.208500
768.312930	67400.779795	33.213517
769.226908	67509.912675	33.218535
770.322836	67616.070131	33.223552
771.002550	67708.610151	33.228570
771.714943	67815.729653	33.233588
772.138108	67933.119928	33.238605
772.835925	68033.333146	33.243623
773.716115	68149.960077	33.248640
774.123777	68262.809285	33.253658
774.531237	68360.265060	33.258676
775.117409	68487.531771	33.263693
776.017437	68591.267247	33.268711
776.310431	68706.261988	33.273728
776.700395	68821.905168	33.278746
777.867175	68941.447927	33.283764
778.632490	69061.367450	33.288781
779.000255	69173.001620	33.293799
779.547469	69306.127787	33.298816
780.092627	69433.881160	33.303834
781.179415	69556.892607	33.308852
781.967929	69704.181457	33.313869
782.571325	69827.192111	33.318887
783.556876	69965.017163	33.323904
784.249016	70096.347756	33.328922
785.342758	70221.208094	33.333940
785.908867	70363.239953	33.338957
786.985651	70482.085515	33.343975
788.141598	70603.099992	33.348992
788.867534	70739.664157	33.354010
790.049825	70855.238191	33.359028
790.495750	70986.463202	33.364045
791.287644	71120.375995	33.369063
792.273557	71242.838504	33.374080
792.596301	71382.520990	33.379098
793.701704	71492.369985	33.384116
794.233422	71631.115409	33.389133
795.199515	71765.850766	33.394151
796.054999	71898.480692	33.399168
796.542640	72035.598347	33.404186
797.414428	72157.800408	33.409204
798.068151	72308.019203	33.414221
798.650397	72434.975098	33.419239
799.931838	72575.917134	33.424256
800.568637	72723.270873	33.429274
801.627743	72848.228184	33.434292
802.222112	72994.338766	33.439309
802.900139	73133.569294	33.444327
803.697164	73271.990638	33.449344
804.212864	73416.637385	33.454362
805.068059	73566.294197	33.459380
806.002926	73710.468988	33.464397
806.873731	73852.676024	33.469415
807.843431	74006.433658	33.474432
808.304537	74149.203543	33.479450
808.937176	74296.669889	33.484468
809.570698	74454.501801	33.489485
810.331203	74598.793508	33.494503
811.697286	74743.220158	33.499520
812.652107	74910.115048	33.504538
813.513744	75039.190245	33.509556
814.428574	75187.204166	33.514573
815.300099	75334.328227	33.519591
816.239698	75464.702151	33.524608
816.422248	75621.687354	33.529626
817.812204	75768.172208	33.534644
818.405244	75904.221859	33.539661
819.122935	76067.136228	33.544679
820.481567	76206.305688	33.549696
821.139723	76349.493825	33.554714
822.167536	76490.996488	33.559732
823.197153	76619.838254	33.564749
823.885037	76760.956079	33.569767
825.077294	76900.157416	33.574784
825.410882	77050.145644	33.579802
826.392394	77188.599362	33.584820
827.026669	77320.249063	33.589837
827.735203	77448.218981	33.594855
828.914899	77584.220111	33.599872
829.443704	77741.694558	33.604890
830.251029	77860.568212	33.609908
831.115136	78000.564360	33.614925
831.839622	78133.007262	33.619943
832.713453	78260.929290	33.624960
833.232580	78399.270876	33.629978
833.924473	78531.183919	33.634996
835.025770	78672.802292	33.640013
835.389720	78823.392079	33.645031
836.495508	78955.738978	33.650048
836.891503	79095.850959	33.655066
837.318060	79246.882357	33.660084
838.032908	79405.678824	33.665101
838.945587	79559.832634	33.670119
839.895731	79728.320809	33.675136
840.889542	79899.181380	33.680154
841.571283	80049.018522	33.685172
842.308616	80207.361544	33.690189
842.800628	80380.509904	33.695207
843.619969	80542.124682	33.700224
844.597170	80713.746946	33.705242
845.438395	80885.740884	33.710260
846.466021	81044.940119	33.715277
847.551226	81212.208932	33.720295
848.575812	81386.535918	33.725312
849.502702	81538.417366	33.730330
850.352388	81697.074939	33.735348
851.289499	81859.698190	33.740365
852.477316	82016.543567	33.745383
853.661874	82183.151594	33.750400
854.443315	82334.556327	33.755418
855.011753	82486.319872	33.760436
856.004339	82658.074569	33.765453
856.405910	82815.719546	33.770471
857.750328	82975.740420	33.775488
858.722229	83136.222486	33.780506
859.939606	83288.130952	33.785524
860.597388	83454.291218	33.790541
861.228367	83608.645725	33.795559
862.445176	83757.678899	33.800576
863.225486	83932.432699	33.805594
863.988134	84074.235832	33.810612
864.949776	84227.881958	33.815629
865.910375	84384.078911	33.820647
866.991879	84536.574850	33.825664
867.708115	84693.339370	33.830682
869.107061	84842.482386	33.835700
869.991834	84994.248310	33.840717
870.472230	85144.835621	33.845735
871.524771	85298.859834	33.850752
872.269515	85455.593201	33.855770
872.862642	85617.116862	33.860788
873.983884	85773.372639	33.865805
874.440397	85929.384917	33.870823
875.083496	86081.906523	33.875840
875.832785	86243.807376	33.880858
877.097174	86402.701155	33.885876
878.036334	86567.856719	33.890893
878.457833	86737.180013	33.895911
879.662998	86896.295747	33.900928
880.887517	87068.589237	33.905946
881.764324	87225.401336	33.910964
882.593113	87374.167596	33.915981
882.908667	87545.545359	33.920999
884.224818	87706.192197	33.926016
885.097434	87857.441012	33.931034
885.961325	88023.840532	33.936052
887.049540	88166.956410	33.941069
887.806757	88335.622070	33.946087
889.150561	88487.227430	33.951104
890.041403	88625.658208	33.956122
891.145743	88760.099669	33.961140
892.314944	88888.639970	33.966157
893.173654	89019.421685	33.971175
893.861449	89164.963726	33.976192
894.988967	89313.477805	33.981210
895.665512	89442.406212	33.986228
896.811954	89577.661696	33.991245
897.126960	89721.142499	33.996263
897.982133	89863.661704	34.001280
899.016138	90016.005152	34.006298
899.812962	90172.223620	34.011316
900.221179	90316.160917	34.016333
900.759014	90475.056679	34.021351
902.234163	90617.370461	34.026368
902.782097	90791.764686	34.031386
903.197384	90951.702726	34.036404
904.155189	91115.248065	34.041421
904.834846	91291.965716	34.046439
905.876367	91469.960243	34.051456
906.468784	91644.169817	34.056474
907.371019	91817.057450	34.061492
908.454000	91989.511451	34.066509
908.985344	92177.936513	34.071527
909.817545	92352.883743	34.076544
910.658303	92550.956300	34.081562
911.471097	92736.079922	34.086580
912.678551	92917.076642	34.091597
913.342858	93111.746342	34.096615
914.745771	93301.156501	34.101632
915.369213	93483.026028	34.106650
916.230153	93682.724770	34.111668
917.584026	93869.343677	34.116685
918.088374	94057.433418	34.121703
919.366495	94251.643830	34.126720
920.628319	94433.117593	34.131738
921.749018	94622.508710	34.136756
922.712088	94797.350718	34.141773
923.675940	94982.004488	34.146791
924.650169	95161.929808	34.151808
925.890802	95333.159987	34.156826
926.674012	95496.365027	34.161844
927.995195	95670.590816	34.166861
928.942069	95847.101358	34.171879
929.779407	96026.074523	34.176896
930.930110	96200.427163	34.181914
932.000456	96361.742253	34.186932
933.350584	96532.120849	34.191949
933.686532	96708.732107	34.196967
934.559258	96864.683719	34.201984
935.575141	97034.779154	34.207002
936.397399	97213.725442	34.212020
937.765568	97385.942651	34.217037
938.810169	97554.422746	34.222055
940.500032	97687.158734	34.227072
941.635877	97843.971945	34.232090
942.395177	98003.918473	34.237108
943.541451	98147.678966	34.242125
943.922854	98313.766923	34.247143
945.110858	98469.144812	34.252160
946.330635	98618.099419	34.257178
946.556130	98792.414137	34.262196
947.264850	98943.062986	34.267213
947.761140	99114.106698	34.272231
948.450553	99284.473974	34.277248
949.325073	99463.908899	34.282266
949.724815	99637.928503	34.287284
950.820596	99810.080792	34.292301
951.544837	99989.056810	34.297319
952.510329	100167.753697	34.302336
953.116320	100336.711112	34.307354
953.711647	100534.983271	34.312372
954.900311	100714.508173	34.317389
955.533592	100905.654703	34.322407
956.346596	101095.994287	34.327424
957.319162	101286.562193	34.332442
958.084926	101494.114013	34.337460
959.743736	101688.667850	34.342477
960.059448	101877.126395	34.347495
961.131727	102070.089552	34.352512
962.260501	102278.448867	34.357530
963.432539	102479.983880	34.362548
964.714754	102666.997076	34.367565
965.525471	102870.348609	34.372583
966.416391	103067.692591	34.377600
967.802225	103264.665124	34.382618
968.291310	103471.290929	34.387636
969.230146	103665.123880	34.392653
970.295840	103872.341511	34.397671
971.366643	104086.429892	34.402688
972.588564	104274.984332	34.407706
973.420079	104472.804749	34.412724
974.593386	104676.648847	34.417741
975.539879	104880.601642	34.422759
976.748257	105082.030663	34.427776
977.966840	105276.272706	34.432794
978.828572	105474.323701	34.437812
979.756570	105667.679487	34.442829
981.001209	105869.811466	34.447847
981.822174	106060.110388	34.452864
983.013212	106255.643362	34.457882
983.707712	106458.845879	34.462900
985.100119	106644.026833	34.467917
986.184764	106848.143126	34.472935
986.923073	107040.425835	34.477952
988.409862	107231.218551	34.482970
989.115717	107432.742256	34.487988
990.079881	107619.938522	34.493005
990.820856	107820.408168	34.498023
992.144615	108020.175173	34.503040
992.700953	108221.957536	34.508058
993.479984	108437.953422	34.513076
994.401480	108640.185288	34.518093
995.276045	108845.985515	34.523111
996.219058	109063.529946	34.528128
997.320113	109270.271317	34.533146
998.436851	109484.953315	34.538164
999.472649	109696.648514	34.543181
1000.141720	109917.652300	34.548199
1001.390358	110128.999107	34.553216
1002.450119	110324.799006	34.558234
1003.552800	110543.190376	34.563252
1004.537081	110749.721732	34.568269
1005.783289	110959.352776	34.573287
1006.854081	111169.698414	34.578304
1008.185119	111369.413146	34.583322
1009.080229	111584.173764	34.588340
1010.141086	111782.251419	34.593357
1011.305659	111987.191698	34.598375
1012.184477	112192.168026	34.603392
1013.223108	112394.028657	34.608410
1014.166470	112599.276065	34.613428
1014.962637	112810.199067	34.618445
1015.727174	113019.710128	34.623463
1016.497960	113227.460929	34.628480
1017.944793	113421.483694	34.633498
1018.734270	113634.073614	34.638516
1019.383375	113826.102704	34.643533
1020.380266	114028.704308	34.648551
1021.129287	114237.137716	34.653568
1022.262390	114440.391262	34.658586
1022.987520	114658.079683	34.663604
1024.078015	114877.369070	34.668621
1025.162064	115094.241535	34.673639
1025.700018	115310.217682	34.678656
1026.995113	115532.240232	34.683674
1027.962368	115755.914959	34.688692
1028.911417	115973.082581	34.693709
1029.827433	116213.429234	34.698727
1030.870180	116444.964545	34.703744
1032.012692	116670.353314	34.708762
1032.890285	116915.666031	34.713780
1033.930950	117141.404784	34.718797
1035.065686	117370.829357	34.723815
1035.976397	117596.327129	34.728832
1037.307480	117824.633358	34.733850
1038.656247	118061.554097	34.738868
1040.271508	118279.744422	34.743885
1041.893114	118497.656629	34.748903
1042.987075	118721.067821	34.753920
1044.231697	118927.997061	34.758938
1044.715065	119156.745324	34.763956
1046.043926	119376.663810	34.768973
1047.034809	119589.620225	34.773991
1047.712966	119817.695386	34.779008
1048.732734	120025.505924	34.784026
1049.859931	120258.832202	34.789044
1051.091047	120495.146250	34.794061
1052.283386	120713.665640	34.799079
1053.153319	120932.987506	34.804096
1054.333657	121150.777235	34.809114
1055.408320	121383.031494	34.814132
1056.990738	121587.782547	34.819149
1057.951449	121813.267098	34.824167
1058.920201	122020.479420	34.829184
1059.739993	122246.573473	34.834202
1060.573894	122481.233161	34.839220
1061.101185	122694.656339	34.844237
1062.278945	122935.636911	34.849255
1063.344878	123184.101858	34.854272
1065.062464	123404.582187	34.859290
1066.027506	123637.797456	34.864308
1066.679490	123874.056958	34.869325
1067.687307	124102.998182	34.874343
1068.625878	124352.190941	34.879360
1069.807572	124577.596765	34.884378
1070.919352	124819.211829	34.889396
1071.935407	125064.773289	34.894413
1072.598434	125293.337008	34.899431
1073.556264	125552.573709	34.904448
1074.856847	125794.076750	34.909466
1075.709393	126039.723866	34.914484
1076.566728	126291.848374	34.919501
1077.949376	126536.600912	34.924519
1078.719603	126792.862910	34.929536
1079.698424	127046.608559	34.934554
1081.073768	127301.190716	34.939572
1081.889983	127572.647786	34.944589
1083.375655	127821.119839	34.949607
1083.993040	128070.687825	34.954624
1085.458687	128326.657794	34.959642
1086.643592	128579.444248	34.964660
1087.697758	128824.117269	34.969677
1088.978501	129063.773672	34.974695
1090.415146	129287.182466	34.979712
1091.527642	129521.065139	34.984730
1092.734049	129753.311679	34.989748
1093.461497	129972.976628	34.994765
1094.757425	130209.774827	34.999783
1095.656235	130448.617726	35.004800
1096.876604	130676.140976	35.009818
1097.738278	130926.959199	35.014836
1098.718680	131157.326839	35.019853
1099.753459	131404.140180	35.024871
1100.849196	131656.624132	35.029888
1102.127114	131901.144951	35.034906
1102.980985	132149.147497	35.039924
1104.380663	132399.318221	35.044941
1105.518213	132640.851034	35.049959
1106.611993	132897.895957	35.054976
1107.648452	133138.080203	35.059994
1108.510111	133389.348971	35.065012
1109.447259	133645.069397	35.070029
1110.699229	133894.743843	35.075047
1111.833254	134161.527955	35.080064
1112.844583	134418.091642	35.085082
1113.868550	134680.004960	35.090100
1114.773528	134957.951169	35.095117
1116.108447	135219.069580	35.100135
1117.019170	135483.999914	35.105152
1117.832081	135754.387148	35.110170
1119.357261	136031.492207	35.115188
1119.922452	136308.707385	35.120205
1121.486254	136574.540306	35.125223
1122.164635	136867.347768	35.130240
1123.403847	137149.859538	35.135258
1124.854375	137423.020506	35.140276
1126.146542	137702.092527	35.145293
1127.736651	137970.163732	35.150311
1128.402984	138236.475174	35.155328
1129.950328	138519.518309	35.160346
1131.905440	138777.976245	35.165364
1133.358491	139022.154178	35.170381
1134.897668	139277.502311	35.175399
1136.162737	139531.528328	35.180416
1137.349006	139782.107931	35.185434
1138.493538	140031.060700	35.190452
1139.254963	140286.595608	35.195469
1140.410812	140541.230511	35.200487
1141.326518	140796.135199	35.205504
1142.248282	141044.358764	35.210522
1143.461582	141305.456408	35.215540
1144.283403	141578.577523	35.220557
1145.584180	141829.622509	35.225575
1146.460025	142103.461641	35.230592
1147.329237	142377.722489	35.235610
1148.673555	142633.026608	35.240628
1149.652274	142907.539880	35.245645
1151.056515	143180.336667	35.250663
1151.933057	143439.363176	35.255680
1154.387267	143685.945360	35.260698
1155.949232	143936.024221	35.265716
1156.945786	144188.975251	35.270733
1158.082980	144438.290916	35.275751
1158.909663	144693.746362	35.280768
1160.081191	144945.596115	35.285786
1161.129987	145212.520173	35.290804
1162.213774	145460.571141	35.295821
1163.369742	145716.283997	35.300839
1164.258885	145990.633369	35.305856
1165.142217	146247.295427	35.310874
1166.189013	146484.060645	35.315892
1167.208583	146744.178491	35.320909
1168.185923	146997.457165	35.325927
1168.980195	147259.873269	35.330944
1170.141525	147532.528271	35.335962
1171.262152	147794.425184	35.340980
1172.229980	148067.382497	35.345997
1173.455747	148336.900512	35.351015
1174.277738	148612.625328	35.356032
1175.358949	148880.966447	35.361050
1176.832285	149165.287935	35.366068
1177.696138	149448.380593	35.371085
1178.809884	149730.838113	35.376103
1179.971795	150020.252608	35.381120
1181.205480	150305.992231	35.386138
1182.789344	150597.079139	35.391156
1183.604740	150890.679576	35.396173
1184.386381	151179.607880	35.401191
1185.861493	151495.121898	35.406208
1187.073448	151786.076592	35.411226
1188.283200	152072.594757	35.416244
1189.894924	152382.880882	35.421261
1191.004348	152672.121752	35.426279
1192.212115	152966.117645	35.431296
1193.295908	153273.822010	35.436314
1195.066530	153558.318284	35.441332
1195.742717	153864.230199	35.446349
1197.158580	154154.268936	35.451367
1198.563817	154457.858251	35.456384
1199.774509	154765.198556	35.461402
1201.117461	155061.179718	35.466420
1202.289618	155364.281927	35.471437
1203.884274	155652.957918	35.476455
1205.242974	155949.640934	35.481472
1206.380629	156244.180933	35.486490
1207.784909	156529.761745	35.491508
1208.741524	156828.230263	35.496525
1210.179029	157118.376442	35.501543
1211.757796	157406.839702	35.506560
1212.635293	157687.289643	35.511578
1213.937661	157981.726696	35.516596
1215.426301	158276.262043	35.521613
1217.028968	158564.755169	35.526631
1218.495041	158851.433528	35.531648
1219.174985	159138.192961	35.536666
1221.220804	159405.510146	35.541684
1222.310109	159695.580387	35.546701
1223.565634	159964.959976	35.551719
1224.806321	160242.297910	35.556736
1225.550520	160522.662856	35.561754
1226.601722	160809.055721	35.566772
1227.675402	161103.705624	35.571789
1229.078393	161381.202132	35.576807
1230.588567	161664.125295	35.581824
1231.790461	161947.469198	35.586842
1232.865211	162218.504679	35.591860
1233.796111	162524.758489	35.596877
1234.777451	162812.369382	35.601895
1235.592730	163117.301846	35.606912
1236.845624	163425.526344	35.611930
1237.963131	163723.321339	35.616948
1238.866341	164041.897271	35.621965
1239.673565	164354.135153	35.626983
1241.137528	164666.634871	35.632000
1242.017666	164992.884913	35.637018
1243.712321	165303.536938	35.642036
1244.931237	165623.785449	35.647053
1245.938469	165941.318062	35.652071
1247.644916	166246.430456	35.657088
1248.463097	166541.871208	35.662106
1249.563200	166846.580407	35.667124
1250.745781	167159.487301	35.672141
1251.895831	167471.475576	35.677159
1253.347255	167779.026206	35.682176
1254.931126	168078.220907	35.687194
1256.013314	168387.816123	35.692212
1257.314635	168705.688308	35.697229
1258.708365	169023.915490	35.702247
1259.776199	169333.608505	35.707264
1260.413450	169652.739051	35.712282
1261.761036	169970.333475	35.717300
1262.946091	170295.367317	35.722317
1264.348482	170625.595515	35.727335
1265.457383	170966.520752	35.732352
1266.634439	171300.470909	35.737370
1267.789697	171630.899479	35.742388
1268.978826	171971.704785	35.747405
1270.314040	172333.692687	35.752423
1271.382772	172671.223769	35.757440
1272.578089	173017.974523	35.762458
1274.370470	173348.576723	35.767476
1275.712795	173704.292697	35.772493
1277.018464	174052.961790	35.777511
1278.503351	174397.060839	35.782528
1279.682521	174744.664580	35.787546
1281.142964	175088.671171	35.792564
1281.853798	175435.697372	35.797581
1283.037329	175775.414517	35.802599
1285.066811	176129.360128	35.807616
1286.241845	176491.038365	35.812634
1288.031435	176824.850566	35.817652
1289.172290	177187.034572	35.822669
1290.571829	177530.561008	35.827687
1292.394632	177862.725011	35.832704
1293.478583	178221.804071	35.837722
1295.076753	178552.563013	35.842740
1296.268493	178903.253053	35.847757
1297.318147	179245.783094	35.852775
1298.698106	179569.629947	35.857792
1299.604043	179915.805339	35.862810
1301.433171	180266.057036	35.867828
1302.888943	180620.192973	35.872845
1303.913037	180964.515729	35.877863
1305.472387	181314.730326	35.882880
1306.479910	181653.323723	35.887898
1308.246123	182009.448735	35.892916
1309.821061	182354.527546	35.897933
1310.752206	182689.764219	35.902951
1312.154439	183037.630261	35.907968
1313.048924	183386.635876	35.912986
1314.230736	183727.016282	35.918004
1315.983405	184071.175878	35.923021
1317.218789	184417.530050	35.928039
1318.623804	184763.414224	35.933056
1320.031581	185121.739092	35.938074
1321.170166	185458.088657	35.943092
1322.495843	185811.494123	35.948109
1323.874956	186165.476942	35.953127
1325.240970	186499.612204	35.958144
1326.403984	186861.365278	35.963162
1328.401920	187212.612525	35.968180
1329.407796	187561.093569	35.973197
1330.447122	187906.258285	35.978215
1331.795203	188251.628039	35.983232
1333.256535	188598.847177	35.988250
1334.531438	188951.138595	35.993268
1335.658048	189283.273638	35.998285
1336.899300	189610.847311	36.003303
1338.862550	189944.244426	36.008320
1339.384317	190277.640192	36.013338
1340.832156	190603.217846	36.018356
1342.706303	190951.297059	36.023373
1343.587090	191289.310791	36.028391
1345.089558	191622.641242	36.033408
1346.255710	191974.283504	36.038426
1347.432871	192314.145638	36.043444
1349.010833	192662.410765	36.048461
1349.669693	193028.703512	36.053479
1351.334162	193375.879459	36.058496
1352.258202	193744.582838	36.063514
1353.669583	194099.878513	36.068532
1355.170890	194460.950254	36.073549
1356.112699	194821.430925	36.078567
1357.589062	195189.823312	36.083584
1359.292029	195555.730333	36.088602
1360.674769	195911.713968	36.093620
1362.169865	196289.592998	36.098637
1363.167904	196661.335626	36.103655
1364.710023	197031.619530	36.108672
1365.754626	197415.025890	36.113690
1367.379260	197785.021216	36.118708
1369.176296	198144.935306	36.123725
1370.724431	198532.264274	36.128743
1372.107227	198900.287231	36.133760
1373.223883	199281.534394	36.138778
1374.399367	199663.815096	36.143796
1375.702550	200034.142727	36.148813
1376.748886	200431.671548	36.153831
1378.053270	200814.851628	36.158848
1379.339123	201213.703975	36.163866
1380.621753	201605.677817	36.168884
1382.635307	201993.000676	36.173901
1384.508734	202370.661490	36.178919
1386.284263	202762.217707	36.183936
1387.234725	203150.763532	36.188954
1388.937414	203519.748882	36.193972
1390.210752	203917.780737	36.198989
1391.381060	204307.337696	36.204007
1392.780109	204685.850893	36.209024
1394.113820	205079.092485	36.214042
1395.698853	205469.514082	36.219060
1396.984905	205857.231839	36.224077
1398.540235	206248.309985	36.229095
1399.864939	206625.969292	36.234112
1401.382574	207019.597091	36.239130
1402.914755	207411.319941	36.244148
1404.409367	207805.336510	36.249165
1405.431786	208200.258347	36.254183
1406.995999	208591.702560	36.259200
1408.140176	208995.026723	36.264218
1409.691355	209383.061398	36.269236
1411.488599	209761.826186	36.274253
1412.631063	210167.607218	36.279271
1414.330592	210559.381622	36.284288
1415.503387	210950.698832	36.289306
1416.805282	211342.466423	36.294324
1418.360434	211726.765787	36.299341
1419.630021	212133.983126	36.304359
1421.174565	212517.513294	36.309376
1422.384383	212921.290426	36.314394
1423.883284	213329.135966	36.319412
1425.515078	213715.857052	36.324429
1426.564497	214121.139270	36.329447
1427.529944	214518.995991	36.334464
1428.980473	214909.155411	36.339482
1430.250276	215300.920971	36.344500
1431.717497	215690.090559	36.349517
1432.780347	216088.420720	36.354535
1434.241514	216482.623323	36.359552
1435.825402	216883.232885	36.364570
1437.713610	217271.450788	36.369588
1439.741054	217654.466216	36.374605
1440.936334	218049.785997	36.379623
1442.224357	218434.780614	36.384640
1444.043990	218840.540682	36.389658
1444.911655	219291.058383	36.394676
1446.857005	219690.121551	36.399693
1447.384568	220093.687184	36.404711
1448.710302	220506.570880	36.409728
1449.766991	220928.517083	36.414746
1451.369840	221347.428665	36.419764
1452.584121	221774.736801	36.424781
1453.906929	222202.536742	36.429799
1455.182376	222631.108188	36.434816
1456.817306	223080.931708	36.439834
1457.809478	223512.652068	36.444852
1459.568716	223964.160447	36.449869
1460.717009	224404.468827	36.454887
1462.167268	224850.316949	36.459904
1464.186192	225296.225369	36.464922
1466.079830	225736.466699	36.469940
1467.886312	226166.411831	36.474957
1469.245370	226601.410701	36.479975
1470.838731	227043.890824	36.484992
1471.992190	227482.304972	36.490010
1473.750452	227927.250271	36.495028
1475.353561	228372.527563	36.500045
1476.225375	228828.468165	36.505063
1477.848774	229263.331164	36.510080
1479.267414	229719.718083	36.515098
1480.668824	230191.933884	36.520116
1482.113792	230648.497451	36.525133
1483.522952	231097.168878	36.530151
1485.249444	231557.168898	36.535168
1486.685846	232024.736922	36.540186
1487.980568	232484.684208	36.545204
1489.943097	232944.319547	36.550221
1491.089369	233411.381105	36.555239
1492.644780	233863.643983	36.560256
1494.377436	234327.385675	36.565274
1495.732102	234791.064125	36.570292
1497.335518	235246.193456	36.575309
1499.119013	235705.256975	36.580327
1501.131939	236165.808011	36.585344
1502.750075	236623.986923	36.590362
1503.953936	237086.960127	36.595380
1506.029025	237529.317081	36.600397
1507.681729	237976.926792	36.605415
1508.686841	238433.992330	36.610432
1510.828361	238884.470222	36.615450
1511.990333	239323.375164	36.620468
1513.602016	239770.868970	36.625485
1515.120094	240244.086079	36.630503
1516.342841	240693.500502	36.635520
1517.968432	241136.727528	36.640538
1519.238071	241594.366461	36.645556
1521.039472	242034.416490	36.650573
1522.296105	242507.300835	36.655591
1523.960707	242952.150889	36.660608
1525.347376	243402.128140	36.665626
1526.531359	243877.364306	36.670644
1528.629055	244320.291092	36.675661
1529.623379	244768.938483	36.680679
1530.906880	245210.223003	36.685696
1532.919995	245635.663656	36.690714
1534.463467	246074.518860	36.695732
1536.124480	246498.926634	36.700749
1537.974246	246947.690500	36.705767
1539.368280	247384.032087	36.710784
1540.886867	247818.600950	36.715802
1542.305965	248270.816387	36.720820
1543.641819	248706.559725	36.725837
1544.623957	249154.860210	36.730855
1545.885291	249613.530393	36.735872
1547.589542	250068.876483	36.740890
1549.121607	250542.490871	36.745908
1550.574065	250998.387645	36.750925
1552.352651	251468.431402	36.755943
1553.338358	251934.770625	36.760960
1555.449438	252405.471774	36.765978
1556.548361	252880.912946	36.770996
1558.040016	253351.640974	36.776013
1559.864551	253844.948690	36.781031
1561.295788	254328.998743	36.786048
1562.878191	254810.636318	36.791066
1563.938319	255302.851933	36.796084
1565.378580	255799.349098	36.801101
1566.917296	256296.490798	36.806119
1568.471133	256805.112542	36.811136
1570.916289	257283.535391	36.816154
1574.727312	257715.854734	36.821172
1576.802131	258180.214804	36.826189
1578.925578	258642.433107	36.831207
1580.448669	259096.494506	36.836224
1582.382680	259530.089329	36.841242
1583.680424	259978.269077	36.846260
1585.247851	260423.584595	36.851277
1586.751993	260880.850123	36.856295
1588.339250	261320.116387	36.861312
1589.959423	261757.776782	36.866330
1590.995160	262218.091691	36.871348
1592.333534	262658.008546	36.876365
1594.022471	263123.728015	36.881383
1594.997985	263589.844507	36.886400
1596.492311	264039.185290	36.891418
1598.020696	264512.805808	36.896436
1599.352106	264989.252975	36.901453
1600.755219	265463.122347	36.906471
1602.145517	265951.981472	36.911488
1603.568527	266432.197803	36.916506
1604.715266	266940.783949	36.921524
1606.259178	267430.861468	36.926541
1607.761168	267944.976884	36.931559
1608.425591	268448.611523	36.936576
1610.348315	268956.000948	36.941594
1611.609065	269490.985198	36.946612
1613.573143	270007.918239	36.951629
1614.898361	270524.473425	36.956647
1616.254899	271049.456589	36.961664
1618.295482	271574.554817	36.966682
1619.647601	272123.720843	36.971700
1621.628021	272645.499684	36.976717
1623.664160	273171.688627	36.981735
1625.213487	273702.377130	36.986752
1627.128520	274214.968453	36.991770
1628.351457	274747.792034	36.996788
1630.326716	275277.721621	37.001805
1631.995038	275795.151966	37.006823
1633.643580	276341.518088	37.011840
1635.359369	276847.736029	37.016858
1636.874379	277368.973528	37.021876
1638.477479	277875.030156	37.026893
1640.051454	278368.490955	37.031911
1641.506953	278889.633332	37.036928
1643.265755	279382.883624	37.041946
1644.628740	279908.204835	37.046964
1646.350461	280423.787361	37.051981
1647.767553	280940.434946	37.056999
1648.705038	281462.926587	37.062016
1650.964922	281987.891259	37.067034
1652.481935	282515.466441	37.072052
1654.238633	283044.219876	37.077069
1656.043624	283575.935811	37.082087
1657.578377	284112.902078	37.087104
1659.373092	284644.768898	37.092122
1660.673789	285199.297453	37.097140
1662.138994	285737.870370	37.102157
1663.780711	286283.016719	37.107175
1664.918232	286842.469057	37.112192
1667.063022	287400.711761	37.117210
1668.941341	287965.067231	37.122228
1670.229495	288524.437765	37.127245
1671.941427	289090.975480	37.132263
1673.911717	289648.019278	37.137280
1675.399673	290215.072090	37.142298
1676.869797	290791.726909	37.147316
1678.306800	291366.378114	37.152333
1680.583425	291952.851843	37.157351
1681.767281	292532.848390	37.162368
1683.904462	293108.925825	37.167386
1685.454668	293693.479446	37.172404
1687.012371	294280.061054	37.177421
1689.156514	294863.672917	37.182439
1690.366192	295448.096492	37.187456
1692.800951	296022.434665	37.192474
1694.645147	296592.066951	37.197492
1696.792950	297172.821932	37.202509
1699.093840	297745.039966	37.207527
1700.690874	298310.691240	37.212544
1702.449587	298871.614120	37.217562
1704.446903	299461.677735	37.222580
1705.668627	300022.225955	37.227597
1707.167454	300588.871839	37.232615
1709.003324	301168.031101	37.237632
1710.849775	301741.775504	37.242650
1712.485950	302328.148662	37.247668
1714.025071	302917.048707	37.252685
1715.930669	303485.236444	37.257703
1717.393066	304062.840186	37.262720
1718.981021	304654.337396	37.267738
1720.884026	305231.886627	37.272756
1722.366845	305815.596819	37.277773
1724.281302	306394.330450	37.282791
1726.116666	306973.124176	37.287808
1728.174488	307567.597830	37.292826
1730.061074	308139.238997	37.297844
1731.709717	308733.365813	37.302861
1733.429915	309316.607202	37.307879
1734.434099	309902.756202	37.312896
1736.004240	310502.699090	37.317914
1738.039156	311089.761623	37.322932
1739.301891	311682.381873	37.327949
1741.114627	312286.283981	37.332967
1742.575651	312881.630653	37.337984
1744.462699	313498.691122	37.343002
1745.997975	314093.533773	37.348020
1747.616554	314703.594603	37.353037
1749.577937	315309.683276	37.358055
1751.318983	315897.596005	37.363072
1752.836675	316491.762349	37.368090
1754.679814	317081.705658	37.373108
1756.518327	317669.105602	37.378125
1758.125006	318260.119392	37.383143
1759.556295	318854.356686	37.388160
1761.615250	319447.495093	37.393178
1763.212947	320042.989843	37.398196
1764.769760	320640.314419	37.403213
1766.768069	321244.518308	37.408231
1768.138264	321860.729104	37.413248
1769.873251	322460.394980	37.418266
1771.906907	323086.032142	37.423284
1773.589163	323701.209431	37.428301
1775.540691	324311.436047	37.433319
1777.343395	324938.236008	37.438336
1779.301411	325561.982727	37.443354
1780.979518	326176.019687	37.448372
1782.560906	326816.446481	37.453389
1784.457064	327443.688354	37.458407
1785.803953	328077.463263	37.463424
1787.375857	328720.182103	37.468442
1789.372162	329355.588280	37.473460
1791.386395	330004.440550	37.478477
1793.214841	330642.348660	37.483495
1795.103291	331298.290638	37.488512
1796.752114	331946.343795	37.493530
1798.780939	332597.703435	37.498548
1800.356982	333258.041112	37.503565
1802.344155	333909.494049	37.508583
1803.663425	334576.763701	37.513600
1805.565282	335238.445803	37.518618
1807.681060	335903.207063	37.523636
1809.325051	336568.926496	37.528653
1811.277391	337238.089965	37.533671
1812.922001	337902.142689	37.538688
1814.763810	338567.474531	37.543706
1816.067008	339251.011047	37.548724
1818.143935	339932.202543	37.553741
1820.077753	340608.230408	37.558759
1822.270780	341287.430218	37.563776
1824.484400	341957.708161	37.568794
1826.314877	342643.701322	37.573812
1828.043525	343315.360949	37.578829
1830.338940	343983.136065	37.583847
1832.123224	344667.661967	37.588864
1833.761539	345337.938161	37.593882
1835.698676	346021.810546	37.598900
1836.914502	346708.507828	37.603917
1839.145036	347376.500420	37.608935
1841.001147	348068.199066	37.613952
1842.625806	348745.154944	37.618970
1844.840071	349421.978290	37.623988
1846.682355	350121.972802	37.629005
1848.906166	350785.044679	37.634023
1850.535595	351465.867767	37.639040
1852.552045	352160.624970	37.644058
1854.553624	352828.550402	37.649076
1856.571083	353509.049893	37.654093
1858.579128	354183.653130	37.659111
1860.482480	354858.237827	37.664128
1862.145377	355537.926746	37.669146
1863.935990	356212.128238	37.674164
1865.912583	356878.777537	37.679181
1867.598247	357559.749982	37.684199
1869.734452	358245.661088	37.689216
1871.447063	358904.887334	37.694234
1873.821414	359562.776053	37.699252
1875.160283	360218.922138	37.704269
1877.254342	360864.961903	37.709287
1879.173613	361523.934437	37.714304
1880.648108	362166.478256	37.719322
1882.697461	362817.213252	37.724340
1884.776131	363476.913944	37.729357
1886.464293	364115.205013	37.734375
1888.259311	364768.791377	37.739392
1890.167824	365418.339774	37.744410
1892.593470	366072.586725	37.749428
1894.189146	366727.948872	37.754445
1895.903508	367375.441578	37.759463
1897.986100	368049.625260	37.764480
1900.299406	368693.014065	37.769498
1902.265397	369348.193921	37.774516
1903.820777	370018.522914	37.779533
1905.815735	370682.273726	37.784551
1907.629819	371350.253104	37.789568
1909.447111	372031.409509	37.794586
1911.382519	372690.695089	37.799604
1912.512775	373376.150182	37.804621
1914.593397	374051.721356	37.809639
1916.483249	374734.717250	37.814656
1918.480031	375428.461453	37.819674
1920.566764	376122.202618	37.824692
1922.152930	376825.269607	37.829709
1924.121711	377512.586374	37.834727
1925.657489	378224.839521	37.839744
1927.456881	378933.610967	37.844762
1929.931509	379631.909848	37.849780
1931.740673	380354.141503	37.854797
1933.813360	381076.365075	37.859815
1935.755847	381782.010760	37.864832
1937.502926	382501.823163	37.869850
1939.184648	383229.567460	37.874868
1940.701893	383968.834589	37.879885
1942.789926	384700.409732	37.884903
1944.610864	385428.995387	37.889920
1946.480379	386191.303377	37.894938
1948.528036	386925.598894	37.899956
1950.286451	387679.624795	37.904973
1951.992128	388438.281169	37.909991
1954.067214	389194.450107	37.915008
1955.688193	389954.453235	37.920026
1957.929317	390723.943647	37.925044
1959.639587	391497.609404	37.930061
1962.135138	392250.339832	37.935079
1964.364144	393018.102411	37.940096
1966.217484	393800.711119	37.945114
1967.955449	394550.037473	37.950132
1970.145567	395332.399205	37.955149
1971.957926	396091.737875	37.960167
1973.709590	396870.253995	37.965184
1975.774198	397652.474600	37.970202
1978.362858	398421.257063	37.975220
1980.415813	399190.488011	37.980237
1981.984446	399965.126046	37.985255
1984.472582	400741.796646	37.990272
1986.245732	401518.969851	37.995290
1988.543199	402293.729629	38.000308
1990.176993	403072.277628	38.005325
1992.095267	403853.696860	38.010343
1994.046423	404635.165176	38.015360
1995.987942	405426.115248	38.020378
1998.342754	406200.429536	38.025396
2000.365008	406970.343272	38.030413
2002.279043	407758.596789	38.035431
2004.263017	408533.717934	38.040448
2006.334287	409298.643647	38.045466
2007.886642	410035.259583	38.050484
2009.790655	410793.660128	38.055501
2011.685207	411546.493161	38.060519
2013.971722	412304.813486	38.065536
2015.877388	413059.806122	38.070554
2018.117449	413824.018450	38.075572
2019.681381	414603.745984	38.080589
2021.638602	415363.629113	38.085607
2023.880035	416129.395475	38.090624
2025.563974	416916.329016	38.095642
2028.052636	417680.843935	38.100660
2029.999366	418463.128384	38.105677
2031.851780	419248.874134	38.110695
2033.952605	420040.252756	38.115712
2035.916774	420820.816194	38.120730
2038.001630	421615.820272	38.125748
2040.175422	422413.443414	38.130765
2042.274201	423196.671185	38.135783
2044.234226	424008.357275	38.140800
2046.209059	424809.937257	38.145818
2048.584375	425602.538351	38.150836
2050.824539	426401.668188	38.155853
2052.529271	427208.505966	38.160871
2054.657248	428010.589045	38.165888
2056.879221	428834.299970	38.170906
2058.570545	429634.527852	38.175924
2060.680296	430445.241128	38.180941
2062.352174	431288.348742	38.185959
2064.365610	432115.676801	38.190976
2066.003451	432945.163975	38.195994
2068.295125	433779.120506	38.201012
2070.504423	434630.422966	38.206029
2072.357283	435466.720045	38.211047
2074.825866	436312.603407	38.216064
2077.027015	437161.486004	38.221082
2079.717833	437992.036568	38.226100
2081.686035	438838.010624	38.231117
2083.892021	439679.511179	38.236135
2086.311862	440520.894567	38.241152
2088.277895	441363.131012	38.246170
2090.121515	442198.828422	38.251188
2092.357236	443054.821454	38.256205
2094.299238	443888.212831	38.261223
2096.621932	444733.754141	38.266240
2098.277134	445602.696693	38.271258
2100.750262	446439.091225	38.276276
2102.976088	447302.458740	38.281293
2104.775968	448161.309242	38.286311
2107.058522	449013.267501	38.291328
2108.850793	449862.895402	38.296346
2111.198860	450722.463642	38.301364
2113.331297	451580.464768	38.306381
2115.213921	452442.771443	38.311399
2117.563687	453311.591216	38.316416
2119.452090	454173.168562	38.321434
2121.912452	455025.917817	38.326452
2124.292843	455881.022062	38.331469
2126.487144	456757.663269	38.336487
2128.686916	457608.377063	38.341504
2130.725332	458476.273578	38.346522
2132.889273	459322.877048	38.351540
2134.912242	460197.477994	38.356557
2137.162977	461057.291715	38.361575
2140.082870	461905.482614	38.366592
2141.742661	462775.481777	38.371610
2144.063447	463623.597631	38.376628
2145.870428	464468.628119	38.381645
2147.499355	465316.330868	38.386663
2150.140000	466130.067337	38.391680
2152.252618	466970.088171	38.396698
2154.205794	467801.558129	38.401716
2156.284043	468636.206374	38.406733
2158.362321	469461.975132	38.411751
2160.593140	470298.143742	38.416768
2162.407863	471155.365336	38.421786
2164.270485	472006.426809	38.426804
2166.140868	472857.499607	38.431821
2168.164773	473729.779465	38.436839
2170.225712	474576.802906	38.441856
2172.010549	475452.781256	38.446874
2173.960776	476344.604225	38.451892
2176.513455	477227.798944	38.456909
2178.368954	478114.097455	38.461927
2180.711946	479017.446416	38.466944
2182.733802	479915.046364	38.471962
2184.762005	480806.641939	38.476980
2186.870687	481730.704080	38.481997
2188.964610	482643.712981	38.487015
2190.970160	483569.314750	38.492032
2192.959029	484503.910347	38.497050
2195.666210	485444.549441	38.502068
2197.709531	486377.220913	38.507085
2199.625295	487326.373682	38.512103
2202.405894	488275.434128	38.517120
2204.542637	489220.057051	38.522138
2206.864186	490152.635557	38.527156
2209.469967	491098.342189	38.532173
2211.322961	492057.749376	38.537191
2214.113769	493000.394915	38.542208
2216.217499	493943.607130	38.547226
2218.257265	494900.252312	38.552244
2221.002273	495849.209177	38.557261
2223.236351	496803.849029	38.562279
2225.221568	497758.980990	38.567296
2227.311143	498719.743174	38.572314
2229.563258	499672.150108	38.577332
2232.597904	500612.518984	38.582349
2235.112224	501579.152000	38.587367
2237.557530	502523.041720	38.592384
2239.686051	503460.070412	38.597402
2242.201938	504410.398131	38.602420
2244.703904	505355.125752	38.607437
2246.476917	506307.584584	38.612455
2249.242641	507249.486729	38.617472
2251.233677	508196.000326	38.622490
2253.235238	509146.440264	38.627508
2255.645506	510095.042710	38.632525
2257.511105	511057.543264	38.637543
2259.957589	512008.597943	38.642560
2262.161473	512963.114232	38.647578
2264.115418	513933.492406	38.652596
2266.645933	514890.913727	38.657613
2268.590673	515853.514361	38.662631
2271.091153	516815.006898	38.667648
2273.558444	517772.011226	38.672666
2275.823151	518736.700031	38.677684
2278.119467	519697.897391	38.682701
2280.546313	520665.110069	38.687719
2283.282300	521628.885947	38.692736
2285.790907	522580.951123	38.697754
2287.705325	523531.896417	38.702772
2290.089450	524485.324297	38.707789
2292.654173	525449.189604	38.712807
2295.136609	526401.070467	38.717824
2297.491319	527332.616267	38.722842
2299.219262	528270.250744	38.727860
2301.508305	529188.296523	38.732877
2303.380521	530121.863233	38.737895
2305.523726	531055.628713	38.742912
2307.759130	531979.552855	38.747930
2309.772740	532908.792114	38.752948
2311.708341	533851.728391	38.757965
2313.947872	534811.014047	38.762983
2316.477899	535756.850336	38.768000
2318.646353	536716.173254	38.773018
2320.289787	537690.265026	38.778036
2323.382135	538644.727931	38.783053
2325.094912	539626.678829	38.788071
2327.492979	540602.210194	38.793088
2330.058239	541594.804169	38.798106
2332.292727	542578.126428	38.803124
2334.464778	543575.828658	38.808141
2336.269463	544579.205175	38.813159
2338.705321	545573.905542	38.818176
2341.571880	546579.629911	38.823194
2344.063252	547594.144775	38.828212
2346.429666	548590.049940	38.833229
2348.616473	549597.528913	38.838247
2351.087866	550619.066689	38.843264
2353.472121	551639.638019	38.848282
2355.454980	552661.205036	38.853300
2358.290573	553678.181629	38.858317
2360.931217	554700.191221	38.863335
2363.213055	555731.179845	38.868352
2366.065895	556756.618046	38.873370
2368.165513	557784.564781	38.878388
2370.554384	558810.324793	38.883405
2372.803310	559855.524824	38.888423
2375.165340	560890.525416	38.893440
2377.447802	561926.664121	38.898458
2379.217735	562977.776070	38.903476
2381.813429	564034.595234	38.908493
2384.211008	565095.681442	38.913511
2386.322181	566146.634037	38.918528
2388.864161	567217.066248	38.923546
2390.941695	568298.232602	38.928564
2393.642272	569362.837384	38.933581
2395.956189	570455.031174	38.938599
2398.205146	571528.317164	38.943616
2400.988314	572606.494958	38.948634
2403.213847	573695.665749	38.953652
2405.433355	574787.554678	38.958669
2408.398661	575870.193214	38.963687
2410.515163	576965.423709	38.968704
2413.252013	578048.464423	38.973722
2415.404325	579134.116668	38.978740
2418.619412	580200.485858	38.983757
2421.210737	581294.556153	38.988775
2424.006878	582361.661297	38.993792
2426.969825	583426.690609	38.998810
2429.048843	584516.396804	39.003828
2431.691092	585574.472197	39.008845
2434.235010	586639.892916	39.013863
2436.542322	587700.897444	39.018880
2438.799933	588768.434724	39.023898
2440.935535	589844.018443	39.028916
2443.564087	590915.314703	39.033933
2445.634041	592008.860013	39.038951
2447.670979	593088.830087	39.043968
2450.463108	594161.011237	39.048986
2452.733919	595257.732874	39.054004
2455.105152	596344.767153	39.059021
2457.154597	597420.633028	39.064039
2459.723697	598480.986859	39.069056
2462.346457	599528.163219	39.074074
2464.473640	600593.857684	39.079092
2467.034231	601648.065564	39.084109
2469.375931	602716.784880	39.089127
2471.769230	603789.702713	39.094144
2474.135873	604851.561061	39.099162
2476.141415	605934.855979	39.104180
2478.147169	607021.451973	39.109197
2480.440663	608111.550589	39.114215
2483.153161	609210.283388	39.119232
2485.932853	610321.208239	39.124250
2488.276492	611436.999007	39.129268
2490.727054	612526.646030	39.134285
2493.109422	613655.367787	39.139303
2495.135096	614773.180047	39.144320
2497.925844	615895.655411	39.149338
2500.011421	617032.386186	39.154356
2502.464957	618170.739624	39.159373
2505.226630	619321.974460	39.164391
2507.461347	620478.624810	39.169408
2510.034263	621631.298049	39.174426
2512.489875	622807.510874	39.179444
2514.647525	623980.996711	39.184461
2517.316025	625163.316199	39.189479
2519.383754	626346.454640	39.194496
2521.777633	627543.098577	39.199514
2524.282816	628765.667393	39.204532
2526.432630	629971.971081	39.209549
2528.974901	631191.508335	39.214567
2531.555902	632412.097471	39.219584
2534.291826	633632.420203	39.224602
2536.501488	634871.211081	39.229620
2539.166118	636105.237902	39.234637
2541.740668	637342.927435	39.239655
2544.619985	638591.449552	39.244672
2547.181595	639825.102566	39.249690
2549.858528	641083.986992	39.254708
2552.215537	642329.549295	39.259725
2554.936237	643579.041018	39.264743
2557.359834	644849.677446	39.269760
2559.938758	646109.906085	39.274778
2562.082987	647371.795377	39.279796
2564.842139	648635.370570	39.284813
2567.886332	649905.221481	39.289831
2570.447811	651177.334352	39.294848
2573.140427	652448.964996	39.299866
2575.336839	653730.930858	39.304884
2578.416943	654998.185460	39.309901
2581.172987	656271.608970	39.314919
2583.567409	657547.119755	39.319936
2586.571464	658820.970083	39.324954
2589.955133	660086.623944	39.329972
2592.974621	661345.600798	39.334989
2595.387524	662602.573068	39.340007
2598.449803	663861.465969	39.345024
2601.223513	665107.549492	39.350042
2603.997035	666349.639639	39.355060
2606.955866	667580.739867	39.360077
2609.651841	668822.472741	39.365095
2612.150210	670063.529346	39.370112
2614.951535	671293.082065	39.375130
2617.058925	672533.631535	39.380148
2619.646374	673761.605589	39.385165
2622.255702	674999.659277	39.390183
2624.322168	676241.616623	39.395200
2627.402955	677478.966707	39.400218
2629.928917	678712.068789	39.405236
2632.310533	679918.889525	39.410253
2635.102334	681117.882527	39.415271
2637.931454	682316.713708	39.420288
2640.448427	683493.233482	39.425306
2643.050568	684702.024936	39.430324
2645.881617	685904.062978	39.435341
2648.627013	687097.613833	39.440359
2650.765154	688309.281231	39.445376
2653.143025	689513.200852	39.450394
2655.651069	690737.985993	39.455412
2658.197770	691951.331462	39.460429
2660.706642	693178.116874	39.465447
2663.082197	694420.584786	39.470464
2665.797266	695632.807989	39.475482
2668.620895	696896.735897	39.480500
2671.136102	698142.827676	39.485517
2674.173810	699386.624373	39.490535
2676.672261	700637.524118	39.495552
2679.496753	701895.678174	39.500570
2682.087420	703165.388563	39.505588
2684.557850	704427.697772	39.510605
2687.139581	705696.198177	39.515623
2689.818598	706985.158779	39.520640
2692.209615	708268.425976	39.525658
2694.869439	709569.289906	39.530676
2697.533215	710867.182627	39.535693
2700.692549	712151.179169	39.540711
2703.156209	713468.022124	39.545728
2705.921399	714784.561965	39.550746
2708.701937	716087.035925	39.555764
2711.285902	717398.595786	39.560781
2714.159241	718721.482121	39.565799
2716.745273	720052.172403	39.570816
2719.150283	721373.876154	39.575834
2721.724422	722719.032399	39.580852
2724.322873	724065.747111	39.585869
2727.283196	725411.688867	39.590887
2729.728511	726770.546318	39.595904
2732.491650	728132.735034	39.600922
2735.188733	729494.807271	39.605940
2737.905834	730852.943713	39.610957
2741.023964	732219.531466	39.615975
2743.804216	733588.513316	39.620992
2746.922344	734943.331378	39.626010
2749.666637	736305.982275	39.631028
2752.248224	737679.240351	39.636045
2755.270844	739055.744285	39.641063
2757.854441	740436.870319	39.646080
2760.596650	741810.230950	39.651098
2763.628895	743187.746090	39.656116
2765.615341	744585.465702	39.661133
2768.828481	745961.678114	39.666151
2771.976311	747350.282697	39.671168
2774.471598	748729.924501	39.676186
2777.710726	750115.508967	39.681204
2780.348129	751491.730637	39.686221
2783.383703	752867.593351	39.691239
2786.312966	754253.820235	39.696256
2789.135280	755630.260337	39.701274
2792.065219	757005.943738	39.706292
2794.861325	758391.298540	39.711309
2797.283205	759761.498739	39.716327
2800.177612	761152.045982	39.721344
2803.180014	762523.916468	39.726362
2806.156792	763902.577947	39.731380
2809.148365	765284.920173	39.736397
2811.828430	766663.075757	39.741415
2814.886541	768021.639769	39.746432
2817.835239	769363.406395	39.751450
2820.480348	770685.220826	39.756468
2822.764852	772020.178071	39.761485
2825.745591	773354.632415	39.766503
2828.195228	774700.871230	39.771520
2830.996247	776024.112468	39.776538
2833.809168	777365.480501	39.781556
2836.113477	778721.858750	39.786573
2839.013610	780077.297373	39.791591
2841.577250	781443.238846	39.796608
2844.257140	782814.399978	39.801626
2846.684995	784190.052602	39.806644
2849.240272	785576.900410	39.811661
2852.649290	786968.293263	39.816679
2855.450943	788365.400016	39.821696
2858.105207	789766.473772	39.826714
2861.187899	791177.053335	39.831732
2863.804196	792600.611999	39.836749
2866.455832	794011.334910	39.841767
2869.228975	795437.382309	39.846784
2872.084717	796877.770771	39.851802
2874.727255	798315.253857	39.856820
2877.365847	799775.549222	39.861837
2880.361996	801221.382598	39.866855
2882.768928	802695.443658	39.871872
2885.315869	804173.864272	39.876890
2888.493553	805662.282742	39.881908
2891.032336	807163.345849	39.886925
2893.876208	808652.637391	39.891943
2896.837935	810165.439441	39.896960
2899.415468	811682.024754	39.901978
2902.563849	813204.724191	39.906996
2905.375017	814735.733695	39.912013
2908.324418	816261.830443	39.917031
2911.481856	817798.483430	39.922048
2914.301339	819338.207567	39.927066
2917.643753	820866.557749	39.932084
2920.113987	822409.972765	39.937101
2923.142552	823956.155964	39.942119
2925.970699	825517.665691	39.947136
2928.447342	827082.227334	39.952154
2931.863100	828654.158288	39.957172
2934.752506	830218.926312	39.962189
2937.888187	831785.129604	39.967207
2941.018986	833361.136964	39.972224
2944.209739	834943.958477	39.977242
2947.158210	836504.570504	39.982260
2949.733642	838079.176305	39.987277
2952.734532	839667.876013	39.992295
2955.367264	841246.900084	39.997312
2957.942514	842832.497731	40.002330
2961.159313	844432.522478	40.007348
2963.844771	846036.994444	40.012365
2967.089363	847637.758202	40.017383
2969.716389	849241.908874	40.022400
2972.786247	850857.331776	40.027418
2975.802505	852461.758114	40.032436
2978.708775	854085.015984	40.037453
2981.872486	855688.681535	40.042471
2985.070931	857307.163070	40.047488
2988.173208	858913.785622	40.052506
2991.498116	860522.376222	40.057524
2993.886425	862147.378777	40.062541
2997.320563	863758.202647	40.067559
3000.051127	865376.372917	40.072576
3002.795517	866991.589362	40.077594
3006.282911	868613.517141	40.082612
3008.929218	870213.355230	40.087629
3012.113377	871803.286207	40.092647
3015.042229	873384.705488	40.097664
3017.757249	874956.547075	40.102682
3021.093182	876518.873110	40.107700
3023.490911	878104.638579	40.112717
3026.428144	879681.960321	40.117735
3029.402921	881276.350487	40.122752
3032.058821	882868.717038	40.127770
3035.291485	884460.651704	40.132788
3037.733193	886075.270563	40.137805
3040.796208	887693.877017	40.142823
3043.896967	889312.025005	40.147840
3046.610094	890947.058542	40.152858
3049.555978	892590.947993	40.157876
3052.376396	894241.910461	40.162893
3055.667692	895888.075967	40.167911
3058.594042	897554.455237	40.172928
3061.778363	899211.051756	40.177946
3064.750820	900874.520422	40.182964
3067.648087	902558.988848	40.187981
3070.803522	904246.087674	40.192999
3074.000942	905939.987204	40.198016
3076.867225	907626.884481	40.203034
3079.855172	909329.988841	40.208052
3082.599276	911048.670535	40.213069
3085.828497	912760.970234	40.218087
3088.862492	914480.266583	40.223104
3092.158363	916217.140167	40.228122
3095.455004	917946.163341	40.233140
3098.110979	919681.849414	40.238157
3101.819877	921418.152025	40.243175
3104.764985	923163.139871	40.248192
3107.951919	924923.255505	40.253210
3111.213126	926658.523297	40.258228
3114.365130	928405.134564	40.263245
3117.518352	930163.057933	40.268263
3120.888265	931899.386463	40.273280
3124.102762	933677.692683	40.278298
3127.163587	935432.834079	40.283316
3130.354624	937188.710052	40.288333
3133.655744	938957.279574	40.293351
3136.755814	940704.149785	40.298368
3139.788324	942475.399684	40.303386
3143.034576	944237.697023	40.308404
3146.360637	946004.541750	40.313421
3149.505654	947767.851894	40.318439
3153.446209	949525.844931	40.323456
3156.919647	951287.321679	40.328474
3160.083135	953032.214764	40.333492
3163.435864	954787.097821	40.338509
3166.945714	956588.285769	40.343527
3170.236995	958369.191927	40.348544
3173.284145	960166.894283	40.353562
3176.609525	961956.659718	40.358580
3179.242193	963759.467338	40.363597
3182.314487	965539.659894	40.368615
3185.560313	967336.752256	40.373632
3188.625309	969163.769631	40.378650
3191.773126	970967.356446	40.383668
3194.607714	972771.891253	40.388685
3197.416897	974572.058690	40.393703
3200.647032	976409.906963	40.398720
3203.571328	978243.999104	40.403738
3206.500255	980058.502743	40.408756
3209.221697	981894.087640	40.413773
3212.355399	983735.635657	40.418791
3215.870254	985578.862462	40.423808
3218.590659	987416.077402	40.428826
3222.584352	989214.454634	40.433844
3225.102986	991030.983084	40.438861
3228.163865	992831.481807	40.443879
3231.410490	994638.279268	40.448896
3234.195195	996447.103557	40.453914
3237.609511	998267.193181	40.458932
3240.847096	1000087.795175	40.463949
3243.939503	1001913.853230	40.468967
3247.462977	1003740.026954	40.473984
3250.465856	1005587.035536	40.479002
3253.666688	1007423.516926	40.484020
3256.719420	1009273.770997	40.489037
3259.559263	1011126.166034	40.494055
3262.847113	1013006.163811	40.499072
3265.675243	1014887.642751	40.504090
3268.726852	1016765.551131	40.509108
3271.832996	1018683.466713	40.514125
3274.728160	1020587.895451	40.519143
3278.493417	1022506.039847	40.524160
3281.468087	1024433.324834	40.529178
3284.826493	1026360.269550	40.534196
3287.886026	1028295.776964	40.539213
3291.176440	1030243.612991	40.544231
3294.522028	1032200.220892	40.549248
3297.309713	1034172.350288	40.554266
3300.955415	1036147.692048	40.559284
3304.225163	1038133.002538	40.564301
3307.218329	1040111.287424	40.569319
3310.722433	1042106.804219	40.574336
3314.216566	1044110.756696	40.579354
3317.854780	1046108.087200	40.584372
3321.441213	1048109.422958	40.589389
3324.664518	1050113.270351	40.594407
3328.285196	1052104.783151	40.599424
3331.338084	1054123.364762	40.604442
3334.668734	1056125.398444	40.609460
3337.771235	1058149.611474	40.614477
3341.153095	1060183.888513	40.619495
3344.476341	1062206.093427	40.624512
3347.701071	1064244.079440	40.629530
3350.953805	1066280.537173	40.634548
3354.244603	1068332.825150	40.639565
3357.219745	1070382.383534	40.644583
3360.611504	1072436.856581	40.649600
3363.897678	1074503.796106	40.654618
3367.265456	1076564.290530	40.659636
3370.448851	1078634.376508	40.664653
3373.428795	1080723.040242	40.669671
3377.458743	1082808.052288	40.674688
3380.425047	1084892.919083	40.679706
3383.517788	1086991.112018	40.684724
3386.812006	1089085.786359	40.689741
3390.078415	1091193.410069	40.694759
3393.429365	1093314.616708	40.699776
3396.746117	1095434.330373	40.704794
3400.108610	1097556.640478	40.709812
3403.495992	1099676.301543	40.714829
3406.512482	1101805.677003	40.719847
3410.046314	1103932.697643	40.724864
3413.697973	1106078.670342	40.729882
3416.990440	1108218.896090	40.734900
3420.713616	1110347.540353	40.739917
3423.972179	1112484.360113	40.744935
3427.987004	1114613.738297	40.749952
3431.310742	1116750.654410	40.754970
3434.786928	1118870.064801	40.759988
3438.469396	1121010.447123	40.765005
3441.168448	1123120.984922	40.770010
3444.514506	1125178.986370	40.775015
3447.806087	1127201.962475	40.780020
3451.050270	1129136.992830	40.785024
3454.289317	1131015.530050	40.790029
3457.069325	1132809.394314	40.795034
3460.445866	1134528.944742	40.800039
3463.442716	1136181.914716	40.805044
3465.909081	1137742.286735	40.810048
3469.125166	1139222.267914	40.815053
3471.496740	1140650.080013	40.820058
3474.514172	1141980.561767	40.825063
3476.523739	1143228.946180	40.830068
3479.025200	1144409.833733	40.835072
3481.368135	1145526.788748	40.840077
3483.439691	1146568.593100	40.845082
3485.586008	1147523.674841	40.850087
3487.680541	1148446.383418	40.855092
3489.595288	1149295.460517	40.860096
3491.207979	1150063.480265	40.865101
3492.931749	1150806.182403	40.870106
3494.636631	1151477.112587	40.875111
3495.818645	1152107.431770	40.880116
3497.513024	1152671.332348	40.885120
3498.695388	1153206.295102	40.890125
3499.876143	1153679.594870	40.895130
3501.002665	1154119.929875	40.900135
3502.402482	1154528.295294	40.905140
3503.427040	1154878.123667	40.910144
3504.527863	1155190.923582	40.915149
3505.097226	1155483.263080	40.920154
3506.474794	1155734.018222	40.925159
3507.122262	1155951.867418	40.930164
3507.818017	1156130.254217	40.935168
3508.782623	1156285.699738	40.940173
3509.312004	1156423.051392	40.945178
3510.055314	1156522.529721	40.950183
3510.702235	1156612.658133	40.955188
3511.346910	1156670.532348	40.960192
3512.125728	1156703.792226	40.965197
3512.611684	1156718.183548	40.970202
3512.967320	1156710.180122	40.975207
3513.343868	1156686.850716	40.980212
3513.794737	1156643.173359	40.985216
3514.586653	1156595.750650	40.990221
3514.613369	1156531.900943	40.995226
3514.861735	1156437.462087	41.000231
3515.366693	1156337.682245	41.005236
3515.417371	1156223.786554	41.010240
3516.054538	1156098.724296	41.015245
3516.250637	1155966.353178	41.020250
3516.395873	1155805.701938	41.025255
3516.889166	1155656.529943	41.030260
3517.435451	1155481.707017	41.035264
3517.874508	1155298.570392	41.040269
3517.571118	1155108.359159	41.045274
3517.809527	1154887.017853	41.050279
3518.199882	1154692.608834	41.055284
3518.495570	1154489.502900	41.060288
3518.675667	1154247.894912	41.065293
3518.662101	1154016.717215	41.070298
3518.922526	1153777.724091	41.075303
3519.077730	1153534.573268	41.080308
3518.939106	1153270.732371	41.085312
3519.485733	1153011.308577	41.090317
3519.227654	1152764.877515	41.095322
3519.873333	1152482.315676	41.100327
3519.533329	1152202.646279	41.105332
3519.688648	1151932.820713	41.110336
3519.894084	1151643.659539	41.115341
3519.751481	1151368.836401	41.120346
3519.997131	1151065.529637	41.125351
3519.986561	1150782.700648	41.130356
3520.313915	1150480.577725	41.135360
3520.340993	1150180.949154	41.140365
3520.211028	1149884.360002	41.145370
3520.243954	1149574.562448	41.150375
3520.420489	1149266.049075	41.155380
3520.181806	1148955.881028	41.160384
3520.726483	1148638.555828	41.165389
3520.743398	1148330.771857	41.170394
3520.939021	1148007.403213	41.175399
3520.869979	1147675.436496	41.180404
3520.834981	1147356.992743	41.185408
3520.994684	1147028.832478	41.190413
3520.518411	1146699.145581	41.195418
3520.756456	1146362.212755	41.200423
3520.428355	1146042.600739	41.205428
3520.651402	1145705.818053	41.210432
3521.122363	1145366.698178	41.215437
3520.535263	1145042.992470	41.220442
3520.895542	1144689.344020	41.225447
3520.934223	1144356.108030	41.230452
3520.958830	1144015.078825	41.235456
3521.108129	1143672.584821	41.240461
3520.966061	1143337.418029	41.245466
3521.163749	1142983.113275	41.250471
3521.112577	1142643.051179	41.255476
3521.055193	1142289.500660	41.260480
3521.176088	1141937.699274	41.265485
3520.728454	1141587.865228	41.270490
3521.267747	1141221.434512	41.275495
3521.243081	1140882.108619	41.280500
3520.951120	1140539.484422	41.285504
3520.970294	1140180.846984	41.290509
3520.700187	1139833.903923	41.295514
3521.136285	1139463.193545	41.300519
3520.790657	1139116.500610	41.305524
3520.805908	1138764.790469	41.310528
3520.721524	1138410.605690	41.315533
3520.884645	1138060.912546	41.320538
3520.809969	1137704.780647	41.325543
3520.870846	1137352.969315	41.330548
3520.718727	1136998.036802	41.335552
3520.486843	1136640.625142	41.340557
3520.551162	1136294.724482	41.345562
3520.715442	1135952.108261	41.350567
3521.004599	1135595.964754	41.355572
3520.519591	1135233.751899	41.360576
3520.682133	1134875.776524	41.365581
3520.577815	1134526.939174	41.370586
3520.953795	1134169.450926	41.375591
3520.478459	1133811.888841	41.380596
3520.346765	1133454.151084	41.385600
3520.645639	1133093.753140	41.390605
3520.256799	1132741.235109	41.395610
3520.219271	1132380.844227	41.400615
3519.871337	1132037.014542	41.405620
3520.063821	1131681.764803	41.410624
3520.220173	1131331.534323	41.415629
3520.394489	1130984.509341	41.420634
3519.918625	1130621.220048	41.425639
3520.256315	1130268.418387	41.430644
3520.255795	1129921.638051	41.435648
3520.537812	1129557.010517	41.440653
3520.009140	1129210.270818	41.445658
3519.859142	1128852.796915	41.450663
3520.068371	1128499.328677	41.455668
3520.162680	1128156.411475	41.460672
3520.108791	1127793.335116	41.465677
3520.045460	1127437.368667	41.470682
3519.921177	1127071.686812	41.475687
3520.034766	1126728.674549	41.480692
3519.852769	1126370.944243	41.485696
3519.685428	1126003.769310	41.490701
3519.614898	1125661.004081	41.495706
3519.814265	1125318.552954	41.500711
3520.069060	1124975.214352	41.505716
3519.538296	1124613.998153	41.510720
3519.787875	1124260.242145	41.515725
3519.921140	1123909.336977	41.520730
3519.660111	1123544.101921	41.525735
3519.904871	1123207.789572	41.530740
3519.878007	1122852.843639	41.535744
3520.058163	1122488.796393	41.540749
3519.582773	1122136.923027	41.545754
3519.615738	1121784.561917	41.550759
3519.471285	1121437.348399	41.555764
3519.115819	1121082.719824	41.560768
3519.516089	1120733.561670	41.565773
3519.515861	1120386.351353	41.570778
3519.416400	1120030.182286	41.575783
3519.412764	1119681.593412	41.580788
3519.294026	1119332.715021	41.585792
3519.398892	1118978.061532	41.590797
3518.989790	1118631.757234	41.595802
3519.059326	1118282.874643	41.600807
3518.966874	1117940.951228	41.605812
3518.993363	1117602.988278	41.610816
3519.014947	1117246.613962	41.615821
3518.644953	1116911.721944	41.620826
3518.612351	1116576.276906	41.625831
3518.549953	1116224.804102	41.630836
3518.531441	1115887.312144	41.635840
3519.251928	1115555.110441	41.640845
3519.132306	1115212.159407	41.645850
3518.710677	1114862.276942	41.650855
3518.989007	1114514.353795	41.655860
3518.636069	1114174.234927	41.660864
3518.874890	1113832.852822	41.665869
3518.438392	1113490.129872	41.670874
3518.523090	1113151.971938	41.675879
3518.280362	1112812.034621	41.680884
3518.165955	1112477.872469	41.685888
3518.318110	1112145.457835	41.690893
3518.224548	1111804.573719	41.695898
3518.266395	1111474.424980	41.700903
3518.284809	1111144.450599	41.705908
3518.097454	1110815.157664	41.710912
3518.527966	1110473.816558	41.715917
3518.197554	1110146.032727	41.720922
3518.189116	1109793.938745	41.725927
3518.196814	1109454.033838	41.730932
3518.075150	1109135.124188	41.735936
3518.198747	1108785.137359	41.740941
3517.838953	1108450.192378	41.745946
3517.848722	1108116.311086	41.750951
3517.982735	1107796.993611	41.755956
3517.779579	1107467.116304	41.760960
3517.847282	1107133.450864	41.765965
3517.868078	1106806.742140	41.770970
3517.948502	1106474.083955	41.775975
3517.531065	1106145.688627	41.780980
3517.573034	1105820.921806	41.785984
3517.963348	1105492.067102	41.790989
3517.301495	1105153.242168	41.795994
3517.698747	1104835.138194	41.800999
3517.258971	1104516.389176	41.806004
3517.299890	1104191.906370	41.811008
3517.766813	1103872.587855	41.816013
3517.467290	1103550.033017	41.821018
3517.943821	1103218.445982	41.826023
3517.640639	1102884.100645	41.831028
3517.433393	1102567.300023	41.836032
3517.481607	1102232.091984	41.841037
3516.967577	1101910.716625	41.846042
3517.307116	1101590.423910	41.851047
3517.412794	1101264.320744	41.856052
3516.997810	1100943.349310	41.861056
3517.491995	1100605.290551	41.866061
3517.185614	1100298.696189	41.871066
3516.889119	1099968.948571	41.876071
3517.061588	1099656.789911	41.881076
3516.869095	1099337.598384	41.886080
3517.086155	1099019.372284	41.891085
3516.873143	1098698.234099	41.896090
3516.889888	1098374.074630	41.901095
3516.985824	1098066.331026	41.906100
3516.993911	1097749.403381	41.911104
3517.138123	1097422.488062	41.916109
3516.684729	1097118.510981	41.921114
3516.768012	1096793.958861	41.926119
3516.901990	1096481.240503	41.931124
3516.721130	1096167.981942	41.936128
3516.482336	1095849.931332	41.941133
3516.709049	1095546.519228	41.946138
3516.154023	1095221.212485	41.951143
3516.245093	1094914.629853	41.956148
3516.093614	1094624.241554	41.961152
3516.605364	1094293.248973	41.966157
3515.992405	1094005.678698	41.971162
3515.932131	1093691.587012	41.976167
3515.734586	1093395.110826	41.981172
3515.635274	1093093.720632	41.986176
3516.106469	1092778.052684	41.991181
3516.176569	1092500.628095	41.996186
3515.967540	1092193.749409	42.001191
3516.051837	1091889.581466	42.006196
3515.726996	1091583.836189	42.011200
3515.809841	1091279.251268	42.016205
3515.683303	1090990.004525	42.021210
3515.867488	1090683.645878	42.026215
3515.658219	1090378.771218	42.031220
3515.873018	1090092.101815	42.036224
3516.000556	1089777.369271	42.041229
3515.822562	1089466.978976	42.046234
3515.720433	1089180.984117	42.051239
3515.867146	1088884.300303	42.056244
3515.236055	1088587.919974	42.061248
3515.634394	1088286.467985	42.066253
3515.444775	1088004.161840	42.071258
3515.453924	1087702.645743	42.076263
3515.529362	1087408.959078	42.081268
3515.298696	1087114.923661	42.086272
3515.659525	1086799.980106	42.091277
3515.044458	1086514.983429	42.096282
3515.527792	1086231.611832	42.101287
3515.070845	1085933.716214	42.106292
3515.117128	1085657.383284	42.111296
3515.039726	1085366.966157	42.116301
3515.102533	1085082.932988	42.121306
3514.965983	1084787.605851	42.126311
3515.169143	1084501.889536	42.131316
3515.018923	1084223.023494	42.136320
3514.859434	1083934.652643	42.141325
3515.048957	1083648.989673	42.146330
3514.923530	1083362.980028	42.151335
3514.716663	1083074.763195	42.156340
3514.694311	1082791.871082	42.161344
3515.051412	1082506.120548	42.166349
3514.887271	1082235.594549	42.171354
3514.619187	1081943.971116	42.176359
3515.026124	1081656.633185	42.181364
3514.604549	1081374.500555	42.186368
3514.389171	1081086.755444	42.191373
3514.262720	1080808.190195	42.196378
3514.600919	1080531.452965	42.201383
3514.471973	1080253.723242	42.206388
3514.351751	1079969.645296	42.211392
3514.787037	1079689.395173	42.216397
3514.735443	1079407.963376	42.221402
3514.298335	1079120.918673	42.226407
3514.324569	1078852.400517	42.231412
3514.369768	1078580.986816	42.236416
3514.368974	1078290.947367	42.241421
3513.962848	1078023.035473	42.246426
3514.106730	1077753.867978	42.251431
3513.914450	1077487.718353	42.256436
3513.945051	1077215.855190	42.261440
3514.185357	1076933.383687	42.266445
3514.017580	1076669.686209	42.271450
3513.748471	1076407.432862	42.276455
3513.822693	1076135.220678	42.281460
3513.696496	1075870.997702	42.286464
3513.872707	1075593.076456	42.291469
3513.685649	1075342.569656	42.296474
3513.837601	1075068.370908	42.301479
3514.040689	1074805.002504	42.306484
3513.621121	1074550.271919	42.311488
3513.843245	1074282.265064	42.316493
3513.423748	1074003.880874	42.321498
3513.603331	1073746.036456	42.326503
3513.509977	1073494.853182	42.331508
3513.530460	1073220.007006	42.336512
3513.651496	1072960.598124	42.341517
3513.442216	1072705.170494	42.346522
3513.420595	1072437.209451	42.351527
3513.837330	1072169.355261	42.356532
3513.264326	1071914.238870	42.361536
3513.256454	1071656.519028	42.366541
3513.268189	1071404.742004	42.371546
3513.039451	1071145.112470	42.376551
3512.894422	1070882.285245	42.381556
3513.039603	1070635.352409	42.386560
3513.039479	1070376.033207	42.391565
3513.142501	1070128.219396	42.396570
3512.639690	1069866.844193	42.401575
3512.998367	1069625.790535	42.406580
3512.578936	1069377.740431	42.411584
3512.683451	1069135.841867	42.416589
3513.024088	1068887.452110	42.421594
3512.773834	1068636.552420	42.426599
3512.978999	1068393.258438	42.431604
3512.639596	1068129.273461	42.436608
3512.716183	1067885.208858	42.441613
3512.792754	1067653.923413	42.446618
3512.379201	1067393.377169	42.451623
3512.648417	1067140.688575	42.456628
3512.562473	1066912.957106	42.461632
3512.433268	1066670.315015	42.466637
3512.721809	1066422.687856	42.471642
3512.429523	1066182.167152	42.476647
3512.594262	1065935.692708	42.481652
3512.155367	1065700.465788	42.486656
3512.673906	1065443.521406	42.491661
3512.312249	1065203.450255	42.496666
3512.396491	1064968.394429	42.501671
3512.542584	1064729.565908	42.506676
3511.940900	1064485.558011	42.511680
3512.280872	1064238.497420	42.516685
3512.521044	1064019.348673	42.521690
3512.473215	1063768.866590	42.526695
3512.323025	1063523.683028	42.531700
3512.181643	1063279.545737	42.536704
3512.274975	1063058.842999	42.541709
3512.170319	1062817.277765	42.546714
3512.160664	1062562.595654	42.551719
3511.980577	1062324.775129	42.556724
3511.663998	1062109.299754	42.561728
3512.022754	1061868.771669	42.566733
3512.146800	1061632.603918	42.571738
3511.909737	1061414.392630	42.576743
3512.131074	1061171.449824	42.581748
3511.692247	1060938.425902	42.586752
3511.981062	1060702.479935	42.591757
3511.623778	1060485.888494	42.596762
3511.620586	1060244.963874	42.601767
3511.927325	1060011.296412	42.606772
3511.630783	1059797.845760	42.611776
3511.763658	1059568.907003	42.616781
3511.362575	1059329.067205	42.621786
3511.602826	1059105.870182	42.626791
3511.790023	1058872.463029	42.631796
3511.499386	1058652.031989	42.636800
3511.685148	1058418.509515	42.641805
3511.567055	1058191.096051	42.646810
3511.481344	1057970.218647	42.651815
3511.751411	1057745.998271	42.656820
3511.572282	1057518.181729	42.661824
3511.407952	1057280.044208	42.666829
3511.413361	1057064.029169	42.671834
3511.170493	1056846.119465	42.676839
3511.436152	1056615.494422	42.681844
3510.997962	1056400.490028	42.686848
3511.299193	1056177.453432	42.691853
3511.095893	1055959.116683	42.696858
3510.784310	1055738.379773	42.701863
3510.917643	1055525.752858	42.706868
3510.723209	1055310.665815	42.711872
3511.145088	1055090.264074	42.716877
3511.119142	1054881.204809	42.721882
3510.648922	1054667.969519	42.726887
3511.150210	1054456.108319	42.731892
3510.626809	1054250.191760	42.736896
3510.740662	1054029.798407	42.741901
3510.873334	1053821.444103	42.746906
3510.749772	1053609.846160	42.751911
3510.954199	1053394.811566	42.756916
3510.990435	1053190.305926	42.761920
3510.858113	1052964.511162	42.766925
3510.831031	1052753.250193	42.771930
3510.543007	1052545.881311	42.776935
3510.460418	1052327.477394	42.781940
3510.787643	1052136.674795	42.786945
3510.668249	1051911.895676	42.791949
3510.752782	1051704.530290	42.796954
3510.509756	1051501.261889	42.801959
3510.727521	1051284.985600	42.806964
3510.837268	1051081.933031	42.811969
3510.950901	1050867.104376	42.816973
3510.684681	1050651.558235	42.821978
3510.733955	1050444.633707	42.826983
3510.932431	1050222.916934	42.831988
3510.690863	1050026.925807	42.836993
3510.680092	1049805.998573	42.841997
3510.382174	1049606.432153	42.847002
3510.388039	1049403.142085	42.852007
3510.609240	1049184.274475	42.857012
3510.475368	1048975.877837	42.862017
3510.300121	1048771.629474	42.867021
3510.348668	1048576.600622	42.872026
3510.193087	1048379.185957	42.877031
3510.444664	1048165.966715	42.882036
3510.451208	1047970.151364	42.887041
3510.305498	1047760.070228	42.892045
3510.522168	1047559.187047	42.897050
3510.378014	1047356.232563	42.902055
3510.211940	1047145.938437	42.907060
3509.856525	1046958.930605	42.912065
3510.104769	1046747.491311	42.917069
3510.142500	1046543.994448	42.922074
3510.118048	1046342.817261	42.927079
3510.101495	1046132.942735	42.932084
3509.838090	1045946.175175	42.937089
3510.240952	1045757.843362	42.942093
3510.160988	1045557.708843	42.947098
3509.958911	1045347.352361	42.952103
3509.920792	1045159.362513	42.957108
3509.719547	1044965.406321	42.962113
3509.874502	1044766.459844	42.967117
3509.787004	1044572.181464	42.972122
3509.353608	1044390.507609	42.977127
3510.033307	1044183.341742	42.982132
3509.424585	1043996.855085	42.987137
3509.452812	1043806.780292	42.992141
3509.276930	1043628.033081	42.997146
3509.220751	1043436.993667	43.002151
3509.691709	1043250.787035	43.007156
3509.535104	1043066.706015	43.012161
3509.300662	1042870.073930	43.017165
3509.369430	1042690.193625	43.022170
3509.447054	1042514.556636	43.027175
3509.433869	1042328.688627	43.032180
3509.371092	1042133.258062	43.037185
3509.359054	1041940.420853	43.042189
3509.425315	1041751.911854	43.047194
3509.389487	1041572.882133	43.052199
3509.768265	1041384.405810	43.057204
3509.498933	1041204.339800	43.062209
3509.502458	1041019.971264	43.067213
3509.161001	1040830.145299	43.072218
3509.012027	1040647.915474	43.077223
3509.419058	1040465.684736	43.082228
3509.049419	1040286.185313	43.087233
3509.422243	1040077.950377	43.092237
3509.474222	1039914.026276	43.097242
3509.261327	1039733.806640	43.102247
3509.168503	1039543.025860	43.107252
3509.084854	1039367.122575	43.112257
3509.106544	1039181.723453	43.117261
3508.895259	1039007.569736	43.122266
3508.696142	1038841.142041	43.127271
3508.748135	1038649.726737	43.132276
3508.771330	1038481.994942	43.137281
3509.055329	1038302.710484	43.142285
3508.992773	1038126.571117	43.147290
3508.306642	1037959.617159	43.152295
3508.732360	1037790.928073	43.157300
3508.731362	1037621.917398	43.162305
3508.762700	1037430.076762	43.167309
3508.931530	1037267.989257	43.172314
3508.521112	1037100.577308	43.177319
3508.841651	1036926.754320	43.182324
3508.815054	1036755.980927	43.187329
3508.495134	1036577.030445	43.192333
3508.439977	1036412.247088	43.197338
3508.399223	1036240.686529	43.202343
3508.697822	1036070.999122	43.207348
3508.373112	1035911.081154	43.212353
3508.154712	1035730.055607	43.217357
3508.395754	1035576.611978	43.222362
3508.050436	1035416.199559	43.227367
3508.148162	1035250.002428	43.232372
3508.317630	1035084.659125	43.237377
3508.262955	1034931.246424	43.242381
3508.662703	1034765.275299	43.247386
3508.228816	1034603.015993	43.252391
3508.493303	1034426.802392	43.257396
3507.837181	1034267.375517	43.262401
3507.969973	1034111.490664	43.267405
3508.262334	1033953.543351	43.272410
3508.135567	1033807.658341	43.277415
3508.176334	1033636.197628	43.282420
3508.032609	1033464.665266	43.287425
3508.394205	1033304.172343	43.292429
3508.311265	1033153.037686	43.297434
3508.398379	1032987.548958	43.302439
3508.575924	1032820.104964	43.307444
3508.072616	1032662.639221	43.312449
3508.220971	1032496.254844	43.317453
3508.219559	1032343.246011	43.322458
3507.870031	1032172.869170	43.327463
3508.075787	1032003.557112	43.332468
3508.197076	1031857.580211	43.337473
3508.262293	1031702.703827	43.342477
3508.021194	1031531.224807	43.347482
3507.916311	1031370.172296	43.352487
3508.168154	1031208.862780	43.357492
3508.150299	1031061.145541	43.362497
3507.854048	1030897.690821	43.367501
3508.004115	1030742.773818	43.372506
3507.778583	1030593.819894	43.377511
3507.942560	1030441.699783	43.382516
3507.997352	1030281.364063	43.387521
3507.718068	1030123.596078	43.392525
3508.127592	1029969.292618	43.397530
3507.646498	1029812.517303	43.402535
3507.926850	1029659.678943	43.407540
3507.461140	1029511.316653	43.412545
3507.850455	1029355.256612	43.417549
3507.884946	1029196.248740	43.422554
3507.523246	1029045.629716	43.427559
3507.520996	1028895.528472	43.432564
3507.720612	1028747.617352	43.437569
3507.714672	1028594.603319	43.442573
3507.966753	1028442.414240	43.447578
3507.542445	1028288.879646	43.452583
3507.677560	1028126.531797	43.457588
3507.283387	1027990.127240	43.462593
3507.363612	1027845.214460	43.467597
3507.425667	1027692.842549	43.472602
3507.307467	1027558.512963	43.477607
3507.342560	1027397.613379	43.482612
3507.718467	1027259.901755	43.487617
3507.631099	1027110.250920	43.492621
3507.664146	1026956.701258	43.497626
3507.566639	1026814.891034	43.502631
3507.474914	1026664.647725	43.507636
3507.163814	1026524.027860	43.512641
3507.517662	1026382.132321	43.517645
3507.431652	1026235.655046	43.522650
3507.303547	1026090.827993	43.527655
3507.590607	1025924.224906	43.532660
3507.472564	1025789.659006	43.537665
3507.212445	1025644.066968	43.542669
3507.669924	1025495.252148	43.547674
3507.631305	1025358.724800	43.552679
3507.617290	1025197.673105	43.557684
3507.500954	1025059.213145	43.562689
3507.518321	1024918.304985	43.567693
3507.464675	1024772.171698	43.572698
3507.302381	1024616.360972	43.577703
3507.321123	1024468.463357	43.582708
3507.250880	1024329.493159	43.587713
3507.142158	1024172.304363	43.592717
3507.300385	1024037.069271	43.597722
3506.992144	1023905.203280	43.602727
3507.057604	1023751.269510	43.607732
3507.190878	1023620.487258	43.612737
3506.893664	1023479.110019	43.617741
3507.146350	1023337.444765	43.622746
3506.999347	1023200.979569	43.627751
3507.034477	1023058.664519	43.632756
3506.949886	1022936.530032	43.637761
3507.002511	1022797.792412	43.642765
3506.896694	1022646.667948	43.647770
3506.683553	1022519.504171	43.652775
3506.857445	1022380.154527	43.657780
3506.435010	1022246.038321	43.662785
3506.897196	1022115.263713	43.667789
3506.687725	1021987.117660	43.672794
3506.543327	1021852.267507	43.677799
3506.478471	1021723.121966	43.682804
3506.941637	1021598.056087	43.687809
3506.597505	1021464.005229	43.692813
3506.456692	1021322.741732	43.697818
3506.484052	1021207.242190	43.702823
3506.846844	1021075.005080	43.707828
3506.668243	1020942.272149	43.712833
3506.256524	1020805.986166	43.717837
3506.479882	1020676.381115	43.722842
3506.620995	1020559.879669	43.727847
3506.636355	1020425.938742	43.732852
3506.449301	1020301.435986	43.737857
3506.031311	1020176.289556	43.742861
3506.225820	1020055.404191	43.747866
3506.132734	1019936.988496	43.752871
3506.350502	1019805.715315	43.757876
3506.178518	1019683.233319	43.762881
3506.173063	1019563.825307	43.767885
3506.249553	1019433.730725	43.772890
3506.096558	1019315.505788	43.777895
3506.412277	1019188.858378	43.782900
3506.309325	1019077.216797	43.787905
3506.188287	1018951.121014	43.792909
3506.414922	1018826.032304	43.797914
3506.204996	1018713.624985	43.802919
3506.279211	1018574.876315	43.807924
3506.078473	1018455.088795	43.812929
3506.291962	1018340.760854	43.817933
3506.441195	1018226.344144	43.822938
3505.790133	1018102.160070	43.827943
3506.271121	1017981.473937	43.832948
3506.211531	1017861.359408	43.837953
3506.198620	1017748.997351	43.842957
3506.529264	1017614.452210	43.847962
3505.834923	1017497.636644	43.852967
3506.297031	1017382.666021	43.857972
3506.115002	1017268.866606	43.862977
3506.028089	1017141.754130	43.867981
3506.082365	1017021.117651	43.872986
3505.701352	1016912.875448	43.877991
3505.989778	1016788.992818	43.882996
3505.731573	1016682.375805	43.888001
3505.835946	1016569.873787	43.893005
3506.065311	1016450.457925	43.898010
3505.728711	1016337.053310	43.903015
3505.732536	1016219.610858	43.908020
3505.776179	1016110.506762	43.913025
3506.030521	1016000.006946	43.918029
3505.991778	1015878.390610	43.923034
3505.780389	1015760.682814	43.928039
3505.999225	1015643.484115	43.933044
3505.843575	1015538.769913	43.938049
3505.504882	1015429.521425	43.943053
3505.712161	1015319.695509	43.948058
3505.440743	1015209.557979	43.953063
3505.614995	1015092.549296	43.958068
3505.429637	1014988.703457	43.963073
3505.430266	1014883.951314	43.968077
3505.753834	1014768.950059	43.973082
3505.647182	1014659.648387	43.978087
3505.537456	1014548.791666	43.983092
3505.756185	1014445.160501	43.988097
3505.537916	1014340.822659	43.993101
3505.621067	1014226.141185	43.998106
3505.385104	1014109.373801	44.003111
3505.645242	1014009.708767	44.008116
3505.866133	1013908.689028	44.013121
3505.746672	1013786.749435	44.018125
3505.616487	1013674.519416	44.023130
3505.363668	1013566.288714	44.028135
3505.459014	1013466.155664	44.033140
3505.615185	1013362.806193	44.038145
3505.157046	1013261.886680	44.043149
3505.462067	1013155.692653	44.048154
3505.276759	1013061.911001	44.053159
3505.522571	1012954.848903	44.058164
3505.636043	1012846.544024	44.063169
3505.438418	1012733.820752	44.068173
3505.409251	1012642.822896	44.073178
3505.151564	1012543.605678	44.078183
3505.617368	1012423.676874	44.083188
3505.465925	1012338.424667	44.088193
3505.409990	1012213.429559	44.093197
3505.354745	1012107.663624	44.098202
3505.073096	1012000.281724	44.103207
3505.469694	1011904.442273	44.108212
3505.331285	1011801.404059	44.113217
3505.270814	1011697.671153	44.118221
3505.445874	1011588.263402	44.123226
3505.160432	1011500.689206	44.128231
3505.459985	1011396.891463	44.133236
3505.156448	1011281.145084	44.138241
3505.367619	1011187.655479	44.143245
3505.333521	1011078.952316	44.148250
3505.175994	1010988.531757	44.153255
3505.284151	1010871.931953	44.158260
3505.404370	1010778.256231	44.163265
3505.170248	1010688.134928	44.168269
3504.872843	1010577.813809	44.173274
3504.685581	1010494.191255	44.178279
3505.004225	1010386.971189	44.183284
3504.893590	1010293.519753	44.188289
3504.753463	1010205.512825	44.193293
3505.081166	1010103.532744	44.198298
3505.057441	1010011.811309	44.203303
3505.245060	1009905.283837	44.208308
3505.134878	1009807.548810	44.213313
3505.242154	1009720.076579	44.218317
3505.191662	1009623.786122	44.223322
3505.213962	1009529.036847	44.228327
3505.501159	1009423.358452	44.233332
3505.432369	1009320.457738	44.238337
3505.328396	1009227.376242	44.243341
3505.456254	1009116.567741	44.248346
3505.211704	1009002.028186	44.253351
3505.222635	1008903.577240	44.258356
3505.222643	1008811.540805	44.263361
3504.839446	1008721.995729	44.268365
3505.001799	1008617.780650	44.273370
3504.644874	1008531.921508	44.278375
3504.954128	1008441.869160	44.283380
3504.745967	1008335.960394	44.288385
3505.103810	1008249.784837	44.293389
3504.905528	1008156.701195	44.298394
3504.843190	1008064.954443	44.303399
3504.823040	1007960.951691	44.308404
3504.830880	1007870.453854	44.313409
3504.561454	1007782.819207	44.318413
3504.966575	1007694.002815	44.323418
3504.860679	1007600.894783	44.328423
3505.094936	1007513.950674	44.333428
3505.090123	1007432.488480	44.338433
3504.699424	1007327.174105	44.343437
3504.843744	1007229.352462	44.348442
3505.126988	1007140.450221	44.353447
3504.864745	1007039.970179	44.358452
3504.861991	1006937.403975	44.363457
3504.639037	1006855.872164	44.368461
3504.979277	1006761.704583	44.373466
3504.363033	1006666.234590	44.378471
3504.772790	1006585.761369	44.383476
3504.896368	1006501.056103	44.388481
3504.383711	1006406.245244	44.393485
3504.916451	1006314.372011	44.398490
3504.482646	1006224.017741	44.403495
3504.788650	1006128.095042	44.408500
3504.529585	1006044.710001	44.413505
3504.404765	1005963.927025	44.418509
3504.624069	1005875.112632	44.423514
3504.493834	1005805.802462	44.428519
3504.586400	1005709.227124	44.433524
3504.618722	1005626.760333	44.438529
3504.352017	1005538.604155	44.443533
3504.621253	1005447.051957	44.448538
3504.736336	1005365.734679	44.453543
3504.476997	1005270.668517	44.458548
3504.353818	1005188.707187	44.463553
3504.512955	1005111.269016	44.468557
3504.425388	1005017.531828	44.473562
3504.315566	1004927.103428	44.478567
3504.376244	1004853.665405	44.483572
3504.345173	1004765.555602	44.488577
3504.077172	1004675.440999	44.493581
3504.208418	1004600.042866	44.498586
3504.207929	1004530.014839	44.503591
3504.111357	1004449.594592	44.508596
3504.171463	1004369.828249	44.513601
3504.218203	1004296.579810	44.518605
3504.566900	1004212.484007	44.523610
3504.237639	1004131.805759	44.528615
3504.157882	1004039.315548	44.533620
3504.418737	1003967.000278	44.538625
3504.326846	1003892.893995	44.543629
3504.189140	1003808.094106	44.548634
3504.126640	1003732.619038	44.553639
3504.426395	1003657.277851	44.558644
3504.192171	1003576.478740	44.563649
3504.023548	1003500.920778	44.568653
3504.368002	1003409.517748	44.573658
3503.920026	1003349.471480	44.578663
3503.834072	1003254.926521	44.583668
3504.186698	1003181.224112	44.588673
3503.911096	1003114.726128	44.593677
3504.222954	1003029.548652	44.598682
3503.956655	1002958.766632	44.603687
3504.162853	1002899.288856	44.608692
3503.717220	1002820.654139	44.613697
3503.822025	1002750.002965	44.618701
3504.150693	1002663.552405	44.623706
3504.180111	1002601.181786	44.628711
3504.100635	1002505.650278	44.633716
3504.003499	1002436.877094	44.638721
3504.031219	1002367.596012	44.643725
3503.986083	1002287.720324	44.648730
3504.018180	1002209.193015	44.653735
3504.115742	1002143.303251	44.658740
3503.986547	1002060.324496	44.663745
3503.962462	1001985.500906	44.668749
3504.203006	1001893.603970	44.673754
3503.724987	1001839.190420	44.678759
3503.696375	1001768.938200	44.683764
3503.739864	1001697.018950	44.688769
3503.869425	1001632.674942	44.693773
3504.296486	1001555.727812	44.698778
3503.792942	1001477.862453	44.703783
3503.847354	1001413.917593	44.708788
3503.932820	1001336.926436	44.713793
3503.970861	1001254.297579	44.718797
3504.038284	1001189.277536	44.723802
3504.110532	1001122.504180	44.728807
3503.843192	1001047.416286	44.733812
3503.753545	1000972.200805	44.738817
3503.654171	1000910.416696	44.743821
3503.897653	1000841.859989	44.748826
3503.411944	1000771.962652	44.753831
3503.439398	1000694.583005	44.758836
3503.763189	1000638.079265	44.763841
3503.733930	1000565.865634	44.768845
3503.688215	1000487.521906	44.773850
3503.651674	1000434.190091	44.778855
3503.099403	1000367.705356	44.783860
3503.542549	1000298.427848	44.788865
3503.417974	1000237.224549	44.793869
3503.778967	1000166.206910	44.798874
3503.350477	1000116.538129	44.803879
3503.412216	1000044.108179	44.808884
3503.534071	999973.127507	44.813889
3503.579788	999924.644362	44.818893
3503.800987	999857.150159	44.823898
3503.757823	999803.716153	44.828903
3503.586600	999727.524131	44.833908
3503.609648	999656.166383	44.838913
3503.506086	999592.226963	44.843917
3503.506851	999522.915492	44.848922
3503.663597	999466.427583	44.853927
3503.717574	999403.141525	44.858932
3503.893172	999335.745972	44.863937
3503.423633	999263.588246	44.868941
3504.302802	999189.260382	44.873946
3504.122421	999123.673309	44.878951
3503.994044	999046.978297	44.883956
3503.916890	998980.301641	44.888961
3503.636761	998911.515739	44.893965
3503.759521	998842.760004	44.898970
3503.544138	998777.564125	44.903975
3503.924680	998698.833358	44.908980
3503.795330	998647.155155	44.913985
3503.508816	998578.560986	44.918989
3503.580986	998505.038628	44.923994
3503.748434	998450.972975	44.928999
3503.499401	998371.367688	44.934004
3503.732413	998307.553064	44.939009
3503.454256	998243.627174	44.944013
3503.605438	998177.585051	44.949018
3503.623680	998118.088004	44.954023
3503.521022	998055.396924	44.959028
3503.965105	997975.866666	44.964033
3503.523420	997930.173221	44.969037
3503.727577	997857.107597	44.974042
3503.771624	997795.460623	44.979047
3503.636695	997731.310604	44.984052
3503.692359	997652.716201	44.989057
3503.594947	997585.344799	44.994061
3503.556416	997518.352429	44.999066
3503.709584	997469.246278	45.004071
3503.649094	997395.633996	45.009076
3503.404224	997326.725651	45.014081
3503.515925	997267.204278	45.019085
3503.437169	997182.684892	45.024090
3503.601212	997128.217633	45.029095
3503.943599	997074.596990	45.034100
3503.688863	997004.615061	45.039105
3503.371069	996945.161048	45.044109
3503.732210	996872.933420	45.049114
3503.199156	996832.602814	45.054119
3503.263791	996750.877808	45.059124
3503.382941	996700.017476	45.064129
3503.346070	996644.896892	45.069133
3503.346432	996571.945673	45.074138
3503.405651	996521.970205	45.079143
3503.572950	996456.684583	45.084148
3503.593238	996393.760070	45.089153
3503.275726	996333.228168	45.094157
3503.376606	996275.061807	45.099162
3503.343008	996217.598835	45.104167
3503.491803	996136.532951	45.109172
3503.555186	996076.325196	45.114177
3503.057106	996027.800867	45.119181
3503.627297	995968.092939	45.124186
3503.341804	995900.245441	45.129191
3503.443219	995849.770049	45.134196
3503.284054	995791.933800	45.139201
3503.059545	995726.509484	45.144205
3503.237277	995666.668201	45.149210
3503.271052	995620.585558	45.154215
3503.440110	995561.134252	45.159220
3503.257331	995497.551330	45.164225
3503.133828	995431.132797	45.169229
3503.306926	995386.486583	45.174234
3503.394932	995324.610668	45.179239
3503.438662	995265.079484	45.184244
3503.446533	995203.312866	45.189249
3503.272775	995143.718807	45.194253
3503.041927	995073.514253	45.199258
3503.120107	995014.754165	45.204263
3503.036398	994970.439254	45.209268
3503.332420	994913.493339	45.214273
3503.135163	994849.613255	45.219277
3503.521663	994797.814984	45.224282
3503.334094	994742.798165	45.229287
3503.140718	994682.520479	45.234292
3503.400577	994617.588181	45.239297
3502.920834	994574.309728	45.244301
3503.178462	994512.104720	45.249306
3503.202050	994459.875970	45.254311
3502.832163	994401.865382	45.259316
3503.105471	994346.963687	45.264321
3502.932199	994298.078732	45.269325
3503.434884	994247.133247	45.274330
3503.105337	994194.375584	45.279335
3502.795102	994140.152641	45.284340
3503.149322	994074.808834	45.289345
3502.816044	994036.861447	45.294349
3503.027660	993969.493625	45.299354
3503.190059	993929.612452	45.304359
3503.140156	993875.928771	45.309364
3503.548171	993817.686640	45.314369
3503.205788	993765.414333	45.319373
3502.848722	993696.480338	45.324378
3502.436333	993655.132736	45.329383
3502.833562	993607.999401	45.334388
3503.561415	993555.938690	45.339393
3503.271830	993499.854664	45.344397
3503.072640	993440.539258	45.349402
3503.173875	993380.199215	45.354407
3502.975127	993322.831579	45.359412
3503.220221	993275.038360	45.364417
3502.832013	993225.497377	45.369421
3503.297768	993153.010287	45.374426
3503.018881	993109.492651	45.379431
3502.825582	993069.371650	45.384436
3502.687013	993028.071836	45.389441
3502.512396	992975.667159	45.394445
3502.898256	992933.987902	45.399450
3502.685525	992886.364282	45.404455
3502.783040	992833.621087	45.409460
3502.931279	992781.843688	45.414465
3502.802966	992746.582897	45.419469
3503.119596	992680.644466	45.424474
3502.900202	992644.423385	45.429479
3502.765788	992589.961735	45.434484
3502.963113	992534.762647	45.439489
3502.402354	992493.918355	45.444493
3502.838484	992442.772732	45.449498
3503.097683	992396.821732	45.454503
3502.768375	992345.996251	45.459508
3502.675739	992284.799263	45.464513
3502.703530	992248.437470	45.469517
3502.666713	992199.122069	45.474522
3502.597564	992143.865600	45.479527
3502.457495	992114.646260	45.484532
3502.736867	992061.670997	45.489537
3502.660318	992027.761884	45.494541
3502.500556	991980.316893	45.499546
3502.512907	991941.518737	45.504551
3502.497519	991891.124871	45.509556
3502.696264	991849.468489	45.514561
3502.235818	991807.043048	45.519565
3502.620784	991762.138493	45.524570
3502.513098	991734.861492	45.529575
3502.808325	991695.137727	45.534580
3502.865579	991638.003351	45.539585
3502.571670	991597.303617	45.544589
3502.922444	991545.676568	45.549594
3502.983411	991493.706841	45.554599
3502.865883	991455.511675	45.559604
3502.693022	991396.852990	45.564609
3502.563937	991366.360650	45.569613
3502.768928	991305.104089	45.574618
3502.668509	991270.414474	45.579623
3502.694205	991227.417181	45.584628
3502.678522	991177.796963	45.589633
3502.812720	991131.271379	45.594637
3502.827770	991091.979520	45.599642
3502.645303	991042.970553	45.604647
3502.534958	990992.584360	45.609652
3502.769530	990949.940544	45.614657
3502.650952	990907.452071	45.619661
3502.575846	990866.126081	45.624666
3502.588007	990816.498124	45.629671
3502.342539	990788.069300	45.634676
3502.536563	990741.140678	45.639681
3502.423373	990691.142278	45.644685
3502.552607	990654.753582	45.649690
3502.472891	990620.739094	45.654695
3502.258792	990567.343689	45.659700
3502.636710	990534.423332	45.664705
3502.477454	990492.425968	45.669709
3502.558459	990436.250636	45.674714
3502.642066	990415.371065	45.679719
3502.549332	990369.364149	45.684724
3502.692413	990325.073130	45.689729
3502.336632	990283.301601	45.694733
3502.375460	990241.659786	45.699738
3502.430331	990207.425642	45.704743
3502.446275	990163.836865	45.709748
3502.523781	990117.214816	45.714753
3502.074540	990094.764167	45.719757
3502.263989	990041.687397	45.724762
3502.072579	990010.808004	45.729767
3502.390174	989982.964990	45.734772
3502.337696	989948.551946	45.739777
3502.136529	989905.972076	45.744781
3502.437494	989858.530997	45.749786
3502.358354	989827.242059	45.754791
3502.155843	989794.217996	45.759796
3502.342450	989759.179336	45.764801
3502.173066	989731.220269	45.769805
3502.336399	989682.727715	45.774810
3502.479241	989631.605139	45.779815
3501.915918	989536.129654	45.784820
3502.277027	989369.114321	45.789825
3502.171735	989163.940858	45.794829
3502.332649	988881.082153	45.799834
3502.374028	988534.440401	45.804839
3502.317177	988128.682542	45.809844
3502.436659	987660.433956	45.814849
3501.885810	987138.013798	45.819853
3502.029151	986528.008313	45.824858
3502.135316	985876.568906	45.829863
3501.891122	985139.327469	45.834868
3501.706705	984340.292546	45.839873
3501.431866	983477.510487	45.844877
3501.442984	982549.621124	45.849882
3501.046699	981539.324174	45.854887
3501.072986	980464.216111	45.859892
3500.574319	979317.089491	45.864897
3500.401574	978099.226631	45.869901
3500.464204	976801.996582	45.874906
3500.328616	975416.031967	45.879911
3499.888526	973961.136679	45.884916
3499.917587	972420.209565	45.889921
3499.467908	970815.743125	45.894925
3499.334194	969122.597123	45.899930
3499.106673	967350.257317	45.904935
3498.842203	965484.833454	45.909940
3498.547292	963546.219110	45.914945
3498.307697	961521.195264	45.919949
3497.665626	959415.531059	45.924954
3497.221249	957231.688108	45.929959
3496.952975	954975.567010	45.934964
3496.943245	952674.269453	45.939969
3496.058508	950310.347721	45.944973
3495.839369	947864.128509	45.949978
3495.449137	945345.026094	45.954983
3494.485610	942736.425718	45.959988
3494.461582	940056.457430	45.964993
3493.557683	937306.278275	45.969997
3493.181686	934456.179852	45.975002
3492.651152	931537.241157	45.980007
3491.676709	928548.252739	45.985012
3491.894404	925467.875731	45.990017
3490.905175	922329.456644	45.995021
3490.522682	919099.779494	46.000026
3489.962518	915781.424729	46.005031
3489.342308	912400.153641	46.010036
3488.594117	908934.368557	46.015041
3488.103715	905393.803538	46.020045
3487.301391	901754.573942	46.025050
3486.361430	898046.144254	46.030055
3486.046811	894282.583291	46.035060
3485.503440	890415.948258	46.040065
3484.855790	886475.661779	46.045069
3484.316437	882436.077364	46.050074
3483.378880	878330.258375	46.055079
3482.270157	874161.644245	46.060084
3482.223441	869892.250547	46.065089
3480.766583	865546.395954	46.070093
3479.849280	861127.610249	46.075098
3479.312015	856623.627965	46.080103
3478.185217	852039.810470	46.085108
3477.572467	847379.828799	46.090113
3476.706802	842645.674618	46.095117
3475.668808	837807.094154	46.100122
3475.001147	832913.030675	46.105127
3473.377161	827939.521129	46.110132
3473.361932	822873.383375	46.115137
3472.298134	817736.572612	46.120141
3471.335854	812513.398866	46.125146
3470.270218	807202.909859	46.130151
3469.092127	801807.799231	46.135156
3468.257705	796341.693460	46.140161
3467.341357	790803.518285	46.145165
3466.072048	785163.892070	46.150170
3465.022573	779450.103317	46.155175
3463.596260	773669.130800	46.160180
3462.653059	767785.536823	46.165185
3461.449787	761834.592407	46.170189
3460.721675	755796.629595	46.175194
3459.645591	749686.670579	46.180199
3458.217057	743489.336075	46.185204
3457.163851	737198.137880	46.190209
3455.753283	730842.723214	46.195213
3454.801189	724393.192270	46.200218
3453.578593	717859.895400	46.205223
3452.088874	711246.246113	46.210228
3450.783208	704547.648114	46.215233
3449.460414	697773.028489	46.220237
3447.793933	690921.462899	46.225242
3446.649473	683991.781542	46.230247
3445.227122	676978.554246	46.235252
3443.784376	669883.196822	46.240257
3442.229118	662722.515546	46.245261
3440.922033	655472.135327	46.250266
3439.362211	648143.947810	46.255271
3437.882321	640753.398568	46.260276
3436.535545	633259.409005	46.265281
3434.533808	625706.842761	46.270285
3433.007585	618074.355326	46.275290
3431.577023	610364.174162	46.280295
3430.155533	602575.929433	46.285300
3428.550976	594715.451884	46.290305
3426.213167	586783.373998	46.295309
3424.935819	578765.361659	46.300314
3423.349717	570672.687285	46.305319
3421.330823	562514.488202	46.310324
3419.806546	554267.856590	46.315329
3417.786696	545954.273417	46.320333
3415.548956	537576.046592	46.325338
3414.154403	529129.459327	46.330343
3412.129388	520600.450765	46.335348
3410.221055	511988.416900	46.340353
3408.055031	503327.735318	46.345357
3406.234382	494588.953173	46.350362
3404.531130	485776.159327	46.355367
3402.067928	476915.898839	46.360372
3400.094486	467967.896673	46.365377
3397.825352	458956.522060	46.370381
3395.650356	449875.117810	46.375386
3393.770116	440729.280241	46.380391
3391.132604	431538.734988	46.385396
3389.227553	422270.351466	46.390401
3386.845387	412943.208452	46.395405
3384.548429	403535.785075	46.400410
3382.315650	394078.960185	46.405415
3379.297994	384561.852260	46.410420
3377.049715	374981.924210	46.415425
3374.208372	365357.090071	46.420429
3371.641701	355675.741236	46.425434
3369.475996	345954.504169	46.430439
3366.277106	336177.807735	46.435444
3363.790581	326334.489357	46.440449
3361.058454	316473.660278	46.445453
3358.138013	306541.178008	46.450458
3355.084865	296575.086713	46.455463
3352.292846	286555.995758	46.460468
3349.141597	276490.251633	46.465473
3345.962212	266404.961729	46.470477
3342.597328	256272.284177	46.475482
3339.696580	246100.362681	46.480487
3336.412765	235910.071743	46.485492
3332.785483	225649.158329	46.490497
3329.415909	215332.444008	46.495501
3325.669905	205058.844180	46.500506
3322.375783	194743.783361	46.505511
3318.008081	184430.684868	46.510516
3314.579846	174100.885132	46.515521
3310.284282	163761.106870	46.520525
3305.957457	153409.050363	46.525530
3302.076481	143059.133405	46.530535
3297.481177	132712.493454	46.535540
3292.964687	122364.202850	46.540545
3287.244861	112037.178419	46.545549
3282.500226	101723.518681	46.550554
3276.954706	91444.231173	46.555559
3270.678232	81216.011608	46.560564
3264.349383	71032.149475	46.565569
3256.953557	60909.827599	46.570573
3248.468223	50888.240639	46.575578
3236.952180	41064.581369	46.580583
3210.621610	31763.551221	46.585588
3174.520928	23017.852074	46.590593
3127.548896	15062.112096	46.595597
3076.048379	7968.591410	46.600602
3018.143827	1952.823008	46.605607
2838.328498	418.206264	46.610612
2682.735852	412.640372	46.615617
2631.047173	391.764384	46.620621
2661.838618	372.374821	46.625626
2733.500033	360.778621	46.630631
2806.550831	363.641588	46.635636
2859.345861	364.619958	46.640641
2886.305727	360.303072	46.645645
2891.861193	354.250606	46.650650
2884.212365	339.798137	46.655655
2872.469218	348.552364	46.660660
2861.333585	349.264154	46.665665
2853.331181	365.790068	46.670669
2849.182953	353.729357	46.675674
2847.882283	337.037211	46.680679
2846.386634	341.470477	46.685684
2845.366324	329.753932	46.690689
2843.527972	334.408848	46.695693
2840.689897	342.636931	46.700698
2838.271391	333.811609	46.705703
2835.327748	328.015056	46.710708
2832.658988	329.981300	46.715713
2829.249321	324.476655	46.720717
2825.410929	323.135135	46.725722
2822.748980	336.262854	46.730727
2820.041145	333.391816	46.735732
2816.665072	329.939057	46.740737
2813.872015	318.621438	46.745741
2810.089188	317.830553	46.750746
2806.785585	307.135889	46.755751
2803.652607	322.972075	46.760756
2800.432998	317.352253	46.765761
2797.653230	309.476221	46.770765
2794.263058	313.205155	46.775770
2791.374339	312.237177	46.780775
2787.521003	305.620426	46.785780
2784.018742	306.378502	46.790785
2780.952453	309.401420	46.795789
2777.123117	306.351846	46.800794
2774.536237	314.709493	46.805799
2771.034150	308.904808	46.810804
2767.835197	300.414302	46.815809
2764.263854	308.007067	46.820813
2760.691275	302.798561	46.825818
2757.724019	295.131346	46.830823
2754.246157	303.573832	46.835828
2751.057191	293.361787	46.840833
2747.371660	292.955741	46.845837
2744.170544	306.197305	46.850842
2740.398506	294.707583	46.855847
2737.490195	295.596048	46.860852
2733.829661	294.395933	46.865857
2730.541533	288.213362	46.870861
2726.681134	287.006938	46.875866
2723.541779	291.754029	46.880871
2719.992510	293.926648	46.885876
2716.875338	290.384002	46.890881
2713.322771	295.144471	46.895885
2709.932728	288.596611	46.900890
2706.784047	284.030559	46.905895
2702.434716	294.543335	46.910900
2699.459108	286.616282	46.915905
2696.703303	285.708610	46.920909
2692.764089	291.031552	46.925914
2689.738029	283.017915	46.930919
2685.739538	299.342604	46.935924
2682.179770	287.165105	46.940929
2678.518229	279.676634	46.945933
2675.710471	283.625976	46.950938
2672.408526	277.012313	46.955943
2668.976789	279.565926	46.960948
2664.824248	284.461643	46.965953
2661.812107	282.638478	46.970957
2658.069012	281.190867	46.975962
2654.796641	278.092545	46.980967
2651.210128	289.140178	46.985972
2647.525614	275.663531	46.990977
2644.282085	283.489570	46.995981
2640.754126	295.671000	47.000986
2637.948046	270.498169	47.005991
2634.390937	284.520519	47.010996
2631.030115	276.213454	47.016001
2627.159801	271.169551	47.021005
2622.998977	285.121757	47.026010
2620.216221	274.483798	47.031015
2617.084993	270.532412	47.036020
2613.874061	283.930208	47.041025
2610.103144	267.502087	47.046029
2606.254797	281.887182	47.051034
2603.182309	267.788938	47.056039
2598.933723	279.905098	47.061044
2595.961372	271.272163	47.066049
2592.371024	271.310835	47.071053
2589.071120	274.575079	47.076058
2585.863383	278.734244	47.081063
2582.407643	267.381809	47.086068
2578.269230	268.964580	47.091073
2574.976995	277.358948	47.096077
2571.315691	268.738604	47.101082
2568.036736	265.058935	47.106087
2564.750505	271.435555	47.111092
2561.437846	260.450820	47.116097
2558.074004	259.075590	47.121101
2554.188454	272.549511	47.126106
2550.808237	264.638844	47.131111
2547.059191	256.859148	47.136116
2543.375285	260.028185	47.141121
2540.363193	261.685705	47.146125
2537.065854	257.400762	47.151130
2533.626293	261.226231	47.156135
2529.998017	263.519099	47.161140
2526.166547	258.669323	47.166145
2522.724868	265.109177	47.171149
2519.302592	262.918527	47.176154
2515.683174	245.394682	47.181159
2512.563036	260.318740	47.186164
2509.249243	249.919367	47.191169
2505.717663	244.777457	47.196173
2502.046241	256.833292	47.201178
2498.341971	253.918442	47.206183
2495.195570	252.892445	47.211188
2491.395294	253.475842	47.216193
2488.091991	254.328113	47.221197
2484.283433	257.056509	47.226202
2481.370589	245.920263	47.231207
2477.635100	251.772042	47.236212
2474.786934	253.991340	47.241217
2470.707041	251.824808	47.246221
2467.367117	249.222028	47.251226
2463.606483	248.125770	47.256231
2459.786952	248.288328	47.261236
2456.539031	243.293431	47.266241
2453.150247	245.325549	47.271245
2449.448728	246.497844	47.276250
2446.302614	243.998670	47.281255
2442.552314	250.485003	47.286260
2439.317621	243.399158	47.291265
2436.032229	244.012510	47.296269
2432.393573	247.517460	47.301274
2428.928238	239.301950	47.306279
2425.081926	243.746920	47.311284
2421.594407	250.548645	47.316289
2418.348780	238.209732	47.321293
2414.812615	249.631710	47.326298
2411.600235	239.514900	47.331303
2407.383226	247.046437	47.336308
2403.906285	245.605480	47.341313
2400.564099	245.218357	47.346317
2397.081468	243.272427	47.351322
2393.986459	235.870856	47.356327
2390.302237	247.503621	47.361332
2387.209929	239.093724	47.366337
2383.836540	238.393190	47.371341
2379.788200	248.094613	47.376346
2376.516861	235.461823	47.381351
2372.848556	252.815869	47.386356
2368.981948	247.699586	47.391361
2365.912213	243.527153	47.396365
2362.139243	247.732850	47.401370
2358.444415	236.766581	47.406375
2355.559553	236.716541	47.411380
2352.039651	244.792758	47.416385
2348.509316	231.843392	47.421389
2344.796509	230.865886	47.426394
2341.472527	235.177787	47.431399
2338.048052	236.100225	47.436404
2334.344438	240.943856	47.441409
2331.086848	227.221235	47.446413
2327.373852	236.122308	47.451418
2324.003395	230.413679	47.456423
2320.535375	233.412737	47.461428
2317.145917	237.567534	47.466433
2313.884101	228.920149	47.471437
2309.881763	227.955191	47.476442
2306.901010	236.823607	47.481447
2302.956047	231.341053	47.486452
2299.169607	233.976699	47.491457
2295.729852	229.093337	47.496461
2292.477854	240.626137	47.501466
2289.023619	235.438636	47.506471
2285.373025	229.663366	47.511476
2281.689933	228.702597	47.516481
2278.764186	233.196669	47.521485
2275.033530	225.318219	47.526490
2271.512112	228.900092	47.531495
2267.905875	235.772950	47.536500
2264.313687	226.319200	47.541505
2261.209343	219.449031	47.546509
2257.292008	235.569715	47.551514
2253.941237	217.643644	47.556519
2250.400895	226.696315	47.561524
2247.341324	220.416826	47.566529
2243.620888	211.843454	47.571533
2239.978488	221.054236	47.576538
2236.793988	234.251606	47.581543
2232.913641	221.729618	47.586548
2229.109139	226.753505	47.591553
2225.899209	227.523993	47.596557
2222.155340	226.285891	47.601562
2219.130376	226.300547	47.606567
2216.009630	225.747447	47.611572
2211.928130	225.349066	47.616577
2208.761649	225.966383	47.621581
2204.870224	234.831525	47.626586
2201.545345	221.991323	47.631591
2198.082991	226.462841	47.636596
2194.707719	216.028818	47.641601
2191.035516	222.872035	47.646605
2187.555985	220.485196	47.651610
2184.131397	219.674022	47.656615
2180.796092	223.431428	47.661620
2176.857738	213.813844	47.666625
2173.233468	218.313656	47.671629
2169.883463	237.921548	47.676634
2166.577915	210.085092	47.681639
2163.185970	219.464434	47.686644
2159.625097	222.975318	47.691649
2156.400504	227.862642	47.696653
2152.452012	229.447951	47.701658
2149.147211	218.020396	47.706663
2145.521154	219.608659	47.711668
2141.970026	222.292974	47.716673
2138.461388	223.442482	47.721677
2134.734641	219.175696	47.726682
2131.582713	219.500495	47.731687
2127.942379	222.890622	47.736692
2124.323057	228.527354	47.741697
2120.928044	227.938932	47.746701
2117.722578	225.968731	47.751706
2114.047845	205.444504	47.756711
2110.248783	225.902995	47.761716
2107.224468	221.809913	47.766721
2103.916358	215.641835	47.771725
2100.039683	223.739402	47.776730
2096.542889	212.948218	47.781735
2092.860573	221.815510	47.786740
2089.723299	232.592576	47.791745
2086.059165	218.886557	47.796749
2082.243501	221.644824	47.801754
2079.074541	220.447120	47.806759
2075.548929	218.857292	47.811764
2072.163541	220.842149	47.816769
2068.755631	211.472962	47.821773
2065.009164	205.027383	47.826778
2061.571369	215.219164	47.831783
2058.099194	216.378380	47.836788
2054.348351	205.769918	47.841793
2051.383726	208.479561	47.846797
2047.649401	214.897513	47.851802
2043.861096	206.786123	47.856807
2040.597386	213.162848	47.861812
2036.989938	216.190849	47.866817
2033.517383	202.207225	47.871821
2029.402275	216.968651	47.876826
2026.536361	211.686217	47.881831
2023.080661	219.235588	47.886836
2019.491213	219.801411	47.891841
2016.091422	210.994244	47.896845
2012.347884	214.573406	47.901850
2009.072937	206.594493	47.906855
2005.612864	216.369792	47.911860
2002.249619	209.527963	47.916865
1998.958325	204.882401	47.921869
1995.168855	221.707296	47.926874
1991.746228	208.322196	47.931879
1987.765554	207.405145	47.936884
1984.122358	209.645670	47.941889
1980.660256	201.372477	47.946893
1977.693130	205.690662	47.951898
1974.191032	215.115175	47.956903
1970.835349	208.188159	47.961908
1967.146596	203.009536	47.966913
1963.497377	206.301164	47.971917
1959.561807	216.444382	47.976922
1956.620775	206.468255	47.981927
1953.563429	206.950076	47.986932
1949.551453	207.300324	47.991937
1946.080075	207.636270	47.996941
1942.515683	218.519846	48.001946
1939.285156	207.618140	48.006951
1935.559631	208.315864	48.011956
1931.582952	211.295515	48.016961
1928.522460	204.925378	48.021965
1924.747676	212.663671	48.026970
1921.569838	211.493746	48.031975
1918.432729	213.805304	48.036980
1914.800213	218.089449	48.041985
1911.251259	213.604036	48.046989
1907.201718	204.910642	48.051994
1903.906042	208.917240	48.056999
1900.629897	213.780508	48.062004
1897.016346	206.543083	48.067009
1893.878416	200.004607	48.072013
1890.054941	206.397379	48.077018
1886.437921	197.842585	48.082023
1883.027061	204.540107	48.087028
1879.414925	199.781403	48.092033
1875.984302	203.375102	48.097037
1872.385625	210.424054	48.102042
1869.273837	203.567943	48.107047
1865.692459	199.205310	48.112052
1862.018588	205.373632	48.117057
1858.458187	196.604999	48.122061
1854.788119	193.168789	48.127066
1851.452432	206.385765	48.132071
1847.752588	203.020471	48.137076
1844.377688	205.467481	48.142081
1841.061631	200.976439	48.147085
1837.360589	195.422953	48.152090
1833.994414	198.850554	48.157095
1830.355124	197.273786	48.162100
1826.748630	196.574386	48.167105
1823.792003	191.709930	48.172109
1820.126326	198.316233	48.177114
1816.686455	199.601345	48.182119
1813.104742	206.623647	48.187124
1809.211706	205.680792	48.192129
1805.665975	200.831459	48.197133
1802.483642	198.999261	48.202138
1799.109362	194.543598	48.207143
1795.400357	201.344410	48.212148
1791.948764	202.597234	48.217153
1788.616130	198.349972	48.222157
1784.777399	210.740560	48.227162
1781.506082	202.991929	48.232167
1777.643328	195.211553	48.237172
1774.319614	202.439223	48.242177
1771.123811	195.575619	48.247181
1767.338170	192.449859	48.252186
1764.370242	193.953389	48.257191
1760.515383	198.927786	48.262196
1756.412569	196.327323	48.267201
1753.429192	193.858052	48.272205
1749.843642	206.372519	48.277210
1746.714651	193.698687	48.282215
1743.155944	198.123052	48.287220
1739.421151	200.379497	48.292225
1736.338294	192.597629	48.297229
1732.163781	194.138271	48.302234
1728.515847	192.960568	48.307239
1725.363798	198.183253	48.312244
1722.083221	197.018830	48.317249
1718.749562	188.230233	48.322253
1715.182019	197.410115	48.327258
1711.572889	191.556618	48.332263
1708.067457	194.016742	48.337268
1703.896919	194.953658	48.342273
1700.795183	189.375157	48.347277
1697.480618	197.164277	48.352282
1693.916794	196.285847	48.357287
1690.621454	193.414460	48.362292
1686.716201	208.518355	48.367297
1683.591493	188.684765	48.372301
1679.839042	188.578772	48.377306
1676.430234	190.557605	48.382311
1672.846025	195.069277	48.387316
1669.172861	197.360772	48.392321
1665.717157	189.736657	48.397325
1662.437045	192.502944	48.402330
1659.025945	193.824718	48.407335
1655.600946	186.346094	48.412340
1651.758215	194.228305	48.417345
1648.379195	193.562097	48.422349
1644.729991	187.991884	48.427354
1641.375425	189.849216	48.432359
1637.900174	192.608746	48.437364
1634.432079	192.977053	48.442369
1630.891003	177.150082	48.447373
1626.942262	188.429358	48.452378
1623.450724	194.317008	48.457383
1620.317075	185.108041	48.462388
1616.963968	191.117084	48.467393
1613.432884	189.769808	48.472397
1609.810713	188.425528	48.477402
1606.838075	182.910123	48.482407
1603.100949	184.316210	48.487412
1599.162818	185.328091	48.492417
1595.549484	189.093732	48.497421
1592.320165	185.835620	48.502426
1588.771691	190.021589	48.507431
1585.447566	189.857885	48.512436
1581.522456	191.500506	48.517441
1578.460055	184.441852	48.522445
1575.093699	181.181601	48.527450
1571.360463	192.096223	48.532455
1567.923533	176.718850	48.537460
1564.125308	170.085699	48.542465
1560.635606	184.305257	48.547469
1557.052030	192.044508	48.552474
1553.862444	185.568405	48.557479
1550.344986	180.727872	48.562484
1546.900983	187.678323	48.567489
1543.553469	177.458449	48.572493
1539.743877	184.827456	48.577498
1536.306380	186.879062	48.582503
1532.655097	181.246514	48.587508
1529.096936	188.644966	48.592513
1525.948112	190.900312	48.597517
1522.308203	180.162813	48.602522
1518.720736	188.406161	48.607527
1515.005555	184.255228	48.612532
1511.423785	180.457370	48.617537
1508.208196	182.787176	48.622541
1504.418027	194.378236	48.627546
1501.690830	177.037229	48.632551
1498.167033	178.595411	48.637556
1494.285589	185.618275	48.642561
1490.841732	184.137292	48.647565
1487.118819	197.322393	48.652570
1483.863691	173.547467	48.657575
1480.656374	194.273082	48.662580
1476.668440	195.414202	48.667585
1473.263736	176.289847	48.672589
1469.635868	178.130603	48.677594
1466.233278	190.282891	48.682599
1462.515256	175.016995	48.687604
1459.027637	186.993108	48.692609
1455.666957	175.160068	48.697613
1452.189239	185.553194	48.702618
1448.469699	188.820266	48.707623
1445.058661	181.529766	48.712628
1441.399697	180.806374	48.717633
1438.528681	176.166425	48.722637
1434.780245	182.095370	48.727642
1431.727628	184.917932	48.732647
1427.770772	172.193494	48.737652
1423.924914	179.596754	48.742657
1420.410673	181.053754	48.747661
1416.808654	173.658255	48.752666
1413.495045	168.049467	48.757671
1410.324158	183.724903	48.762676
1406.733416	180.054468	48.767681
1403.215802	176.128484	48.772685
1399.468506	187.238564	48.777690
1395.967503	184.102244	48.782695
1392.380186	178.980321	48.787700
1389.124652	185.766841	48.792705
1386.160086	178.894680	48.797709
1382.447449	184.917384	48.802714
1378.808948	182.784210	48.807719
1375.527361	176.360683	48.812724
1371.379903	179.442902	48.817729
1368.365754	167.817221	48.822733
1364.223904	169.942643	48.827738
1360.907115	167.028893	48.832743
1357.710832	175.045546	48.837748
1354.192035	175.969603	48.842753
1350.753890	171.928128	48.847757
1347.286233	179.953767	48.852762
1343.424002	175.486549	48.857767
1340.009585	178.133572	48.862772
1336.181527	179.396069	48.867777
1333.387188	172.956464	48.872781
1329.568120	170.233862	48.877786
1325.980393	164.189225	48.882791
1322.987062	160.955341	48.887796
1318.983673	179.542212	48.892801
1315.574088	168.240507	48.897805
1311.978359	169.667207	48.902810
1308.736798	170.081744	48.907815
1305.217055	173.766071	48.912820
1301.546846	166.990212	48.917825
1298.257515	164.931155	48.922829
1294.337230	173.351072	48.927834
1290.796432	167.407328	48.932839
1287.382132	168.649894	48.937844
1284.149396	170.697611	48.942849
1280.993406	172.265428	48.947853
1277.527727	166.200771	48.952858
1274.006524	163.680409	48.957863
1269.746201	172.214872	48.962868
1266.435336	172.503441	48.967873
1262.781302	160.454756	48.972877
1259.323562	163.344852	48.977882
1256.318865	164.680923	48.982887
1252.328127	158.530408	48.987892
1248.731293	167.009024	48.992897
1245.842681	168.961575	48.997901
1242.156800	163.697179	49.002906
1238.440686	165.309925	49.007911
1234.883672	170.229093	49.012916
1231.336915	161.645852	49.017921
1228.201464	168.679766	49.022925
1224.593227	170.936295	49.027930
1220.917197	165.734904	49.032935
1217.514597	163.738092	49.037940
1213.816172	165.079884	49.042945
1210.389665	163.771297	49.047949
1206.840059	170.542795	49.052954
1203.279283	172.773546	49.057959
1200.416613	157.294040	49.062964
1196.205986	177.283419	49.067969
1192.782084	169.156719	49.072973
1189.594923	168.955896	49.077978
1185.720334	165.490888	49.082983
1182.609022	166.289950	49.087988
1179.053454	166.832350	49.092993
1175.844141	166.604212	49.097997
1171.981439	170.124230	49.103002
1168.140794	162.078876	49.108007
1164.727573	167.552557	49.113012
1161.409301	167.353463	49.118017
1158.279622	161.617868	49.123021
1154.778308	179.101522	49.128026
1150.736614	167.806406	49.133031
1147.396823	154.336192	49.138036
1144.056803	164.643948	49.143041
1140.325121	165.245630	49.148045
1136.790177	163.006312	49.153050
1133.365783	165.959331	49.158055
1129.899355	165.517159	49.163060
1126.058479	173.754656	49.168065
1122.902390	167.136721	49.173069
1119.461974	167.091886	49.178074
1115.743415	173.688680	49.183079
1112.537779	163.818369	49.188084
1109.099401	163.402554	49.193089
1105.282252	170.476843	49.198093
1102.091595	173.270042	49.203098
1098.350750	171.867397	49.208103
1094.601573	165.350847	49.213108
1091.362100	173.379170	49.218113
1088.297745	163.837255	49.223117
1084.591252	170.027584	49.228122
1080.656657	167.222586	49.233127
1077.333878	164.555131	49.238132
1073.787234	172.845197	49.243137
1070.045755	167.270241	49.248141
1066.659433	162.171265	49.253146
1063.461633	170.561097	49.258151
1060.407259	164.479466	49.263156
1056.449440	170.728567	49.268161
1053.150703	163.441859	49.273165
1049.230630	160.514520	49.278170
1045.325819	168.531755	49.283175
1042.164706	160.515073	49.288180
1038.661774	165.233320	49.293185
1035.727879	167.755965	49.298189
1032.179859	170.137216	49.303194
1028.599755	156.907811	49.308199
1024.792086	156.489675	49.313204
1021.104293	163.121386	49.318209
1017.551684	164.374785	49.323213
1014.298596	165.802679	49.328218
1011.036107	168.299085	49.333223
1007.575799	167.655497	49.338228
1003.935013	161.815247	49.343233
1000.734455	162.339869	49.348237
996.702786	168.649633	49.353242
992.934262	170.895749	49.358247
989.803319	156.364543	49.363252
986.147787	172.535056	49.368257
983.009643	156.556980	49.373261
979.109412	156.136296	49.378266
975.444967	163.394384	49.383271
972.335957	158.062625	49.388276
968.437945	165.246124	49.393281
964.997473	161.528343	49.398285
961.757947	162.596200	49.403290
958.028760	172.195029	49.408295
954.869679	162.329850	49.413300
951.908328	158.554177	49.418305
948.113369	157.604010	49.423309
944.627280	170.875692	49.428314
940.615390	167.229780	49.433319
937.186485	164.003676	49.438324
933.194114	167.527670	49.443329
930.037804	158.476351	49.448333
926.514359	157.439534	49.453338
923.371150	163.596813	49.458343
920.004370	154.664901	49.463348
916.264959	169.593110	49.468353
912.780507	168.633718	49.473357
909.404011	162.996030	49.478362
905.441519	165.910843	49.483367
902.451869	159.498374	49.488372
898.272932	160.023789	49.493377
895.410333	165.948582	49.498381
891.462040	164.376292	49.503386
888.172915	172.003770	49.508391
885.177254	157.385769	49.513396
881.352817	160.603754	49.518401
877.433904	153.477075	49.523405
873.868811	152.456142	49.528410
870.570756	166.798480	49.533415
867.152310	158.299347	49.538420
863.600657	166.792769	49.543425
860.457809	167.348080	49.548429
856.783978	164.665507	49.553434
853.022084	166.353694	49.558439
849.945422	154.633474	49.563444
846.266242	160.066962	49.568449
842.742628	150.328644	49.573453
839.325818	151.897307	49.578458
835.165428	160.960860	49.583463
832.249415	154.984755	49.588468
828.734674	151.505532	49.593473
825.338040	158.576611	49.598477
822.140619	161.085344	49.603482
818.058217	155.886192	49.608487
814.337322	150.998586	49.613492
810.912565	165.280081	49.618497
807.362735	153.690904	49.623501
803.866360	156.384960	49.628506
800.234780	150.419605	49.633511
797.618146	149.786959	49.638516
793.830246	161.953183	49.643521
790.206930	153.900012	49.648525
786.650712	158.645231	49.653530
782.769941	163.165348	49.658535
779.596979	158.854084	49.663540
775.883926	165.960768	49.668545
772.792229	164.772330	49.673549
769.268752	162.357392	49.678554
765.377199	157.297628	49.683559
762.060782	162.061661	49.688564
758.367043	166.639300	49.693569
755.018213	151.506227	49.698573
751.877264	149.065913	49.703578
748.251229	155.274978	49.708583
744.701304	153.053841	49.713588
741.120797	162.919044	49.718593
737.596191	148.082764	49.723597
733.903746	151.960242	49.728602
729.914306	164.268597	49.733607
726.975307	162.210574	49.738612
723.461985	156.877843	49.743617
719.928745	166.258748	49.748621
717.036713	168.103954	49.753626
712.903147	164.979451	49.758631
709.646890	151.850489	49.763636
706.147179	168.963271	49.768641
702.440300	150.763384	49.773645
699.004601	147.835192	49.778650
695.432824	156.798152	49.783655
692.136069	155.119861	49.788660
688.503973	164.032511	49.793665
684.780120	161.042703	49.798669
681.649236	158.580438	49.803674
677.800657	156.199218	49.808679
674.823424	163.959655	49.813684
671.340399	151.864781	49.818689
667.411123	148.352599	49.823693
663.955790	161.609435	49.828698
660.355215	150.128282	49.833703
657.108977	149.300457	49.838708
653.365042	159.776823	49.843713
649.679407	148.960158	49.848717
646.354861	152.341851	49.853722
642.794535	163.710914	49.858727
639.472430	146.902493	49.863732
635.923372	143.979247	49.868737
632.658127	145.839464	49.873741
629.133550	144.705131	49.878746
625.665514	154.283364	49.883751
621.895307	156.164145	49.888756
618.707073	159.027696	49.893761
614.900292	153.494890	49.898765
611.179755	152.509148	49.903770
607.356448	158.627250	49.908775
604.473026	150.885878	49.913780
601.092694	150.410130	49.918785
597.626913	151.156526	49.923789
593.554138	151.322166	49.928794
590.037885	149.999134	49.933799
586.991146	153.359732	49.938804
583.463782	157.201834	49.943809
580.207531	153.496560	49.948813
576.437741	147.730370	49.953818
572.932205	153.471230	49.958823
569.622964	145.338804	49.963828
565.989572	152.845988	49.968833
562.629892	145.147000	49.973837
559.042291	151.503512	49.978842
555.225397	160.540763	49.983847
552.029510	141.878553	49.988852
548.247837	150.069842	49.993857
544.235722	156.302329	49.998861
541.142895	152.921096	50.003866
537.589994	154.681779	50.008871
534.338604	147.798059	50.013876
530.532368	150.167066	50.018881
527.646420	139.360858	50.023885
524.384756	143.675062	50.028890
520.635725	151.426005	50.033895
516.995283	134.599627	50.038900
512.917884	152.323254	50.043905
509.665822	151.327470	50.048909
506.485153	141.507568	50.053914
502.630196	152.717288	50.058919
499.052403	146.725676	50.063924
495.757487	147.720035	50.068929
492.445347	151.014513	50.073933
489.062450	132.867940	50.078938
485.239479	145.258700	50.083943
481.967823	143.312770	50.088948
478.518416	144.324567	50.093953
474.749539	143.882585	50.098957
471.521693	142.868220	50.103962
467.729101	148.768816	50.108967
464.187972	143.622658	50.113972
460.572586	146.256141	50.118977
457.392469	148.026219	50.123981
454.039316	150.291025	50.128986
450.448497	142.150630	50.133991
446.831210	140.885507	50.138996
443.015540	147.306977	50.144001
439.579944	151.167533	50.149005
436.339206	139.102156	50.154010
432.263148	148.999232	50.159015
429.390659	131.820044	50.164020
425.772786	145.412105	50.169025
422.202758	145.925527	50.174029
419.034811	141.058108	50.179034
415.329000	147.826367	50.184039
412.033197	142.635570	50.189044
408.142163	141.810014	50.194049
404.822615	150.048744	50.199053
401.440908	137.825845	50.204058
397.324503	149.364211	50.209063
394.198169	144.472467	50.214068
390.776408	145.181018	50.219073
387.157154	136.446827	50.224077
383.719646	147.925332	50.229082
379.977353	140.931511	50.234087
376.656658	146.920034	50.239092
373.277251	141.821403	50.244097
369.846585	140.467486	50.249101
366.035791	133.257399	50.254106
362.212254	143.879533	50.259111
359.288792	134.568119	50.264116
355.638957	149.618574	50.269121
351.998319	143.000227	50.274125
349.109945	141.022911	50.279130
344.948822	154.596932	50.284135
341.687869	134.842867	50.289140
338.280101	137.230895	50.294145
334.586628	142.339562	50.299149
330.954949	133.233859	50.304154
327.129185	142.479162	50.309159
324.098838	141.442899	50.314164
320.782112	140.161242	50.319169
317.226560	135.479261	50.324173
313.797822	144.102963	50.329178
310.251907	139.774056	50.334183
306.763603	141.481471	50.339188
303.350990	134.796284	50.344193
299.672717	132.262861	50.349197
296.421202	131.541358	50.354202
292.503509	151.833205	50.359207
289.553530	143.653826	50.364212
285.651650	129.811511	50.369217
282.034376	142.561615	50.374221
278.492429	142.659976	50.379226
274.726490	149.174142	50.384231
271.515595	141.424410	50.389236
267.944494	142.308738	50.394241
264.587617	145.535838	50.399245
261.513513	140.571314	50.404250
257.459781	144.339245	50.409255
254.360078	137.045385	50.414260
250.717645	144.878685	50.419265
247.052901	138.920441	50.424269
243.537902	134.182281	50.429274
239.933571	142.749099	50.434279
236.393688	130.306504	50.439284
232.920539	135.333142	50.444289
229.319398	137.481087	50.449293
226.256977	133.542435	50.454298
222.425087	136.859876	50.459303
219.133140	134.299567	50.464308
215.412978	142.895597	50.469313
211.840630	148.556513	50.474317
209.107631	130.021500	50.479322
204.992202	147.347947	50.484327
201.545673	142.773805	50.489332
197.919597	137.281660	50.494337
194.632591	134.509526	50.499341
191.292369	138.357403	50.504346
187.161452	131.780912	50.509351
184.409227	138.173399	50.514356
180.637428	137.002822	50.519361
176.855442	138.108305	50.524365
173.454828	139.722477	50.529370
169.907128	133.205702	50.534375
166.392455	138.691664	50.539380
162.644591	135.462076	50.544385
158.912944	139.790671	50.549389
156.188467	135.872080	50.554394
152.308578	143.558207	50.559399
149.057722	133.423381	50.564404
145.862486	139.279500	50.569409
141.957448	139.820416	50.574413
138.439278	131.792233	50.579418
134.724847	123.635583	50.584423
131.675200	132.345686	50.589428
128.177150	132.872731	50.594433
124.589204	138.361351	50.599437
121.501730	138.102057	50.604442
117.097610	134.619175	50.609447
114.142652	133.441122	50.614452
110.542953	132.065165	50.619457
106.830631	127.551776	50.624461
103.412581	139.774974	50.629466
99.735124	138.500561	50.634471
96.388417	129.863197	50.639476
92.840403	144.483272	50.644481
89.044528	136.300938	50.649485
85.909060	139.353224	50.654490
82.726159	144.940673	50.659495
79.229236	132.482010	50.664500
75.490474	140.911102	50.669505
71.575839	135.079012	50.674509
68.368464	126.011892	50.679514
64.355222	144.442915	50.684519
61.437322	132.960259	50.689524
58.077576	131.946103	50.694529
54.721917	137.634030	50.699533
51.169284	132.093735	50.704538
47.355450	138.777429	50.709543
44.045915	135.508234	50.714548
40.288354	137.448124	50.719553
36.681840	135.007081	50.724557
33.555332	140.492004	50.729562
29.885426	135.175908	50.734567
26.302032	132.736576	50.739572
22.908380	141.133524	50.744577
19.337084	137.535379	50.749581
16.190204	128.959948	50.754586
11.936003	134.444980	50.759591
8.310909	134.046106	50.764596
5.128362	130.259324	50.769601
1.756199	135.352356	50.774605