Thu Jun 16 11:16:41 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.351518	84.131476	0.000000
0.266587	92.792529	0.005005
0.357096	97.216415	0.010010
0.403955	95.666526	0.015014
0.011790	97.521223	0.020019
0.730368	96.552484	0.025024
0.239025	81.270731	0.030029
0.020961	85.712460	0.035034
-0.085834	58.589107	0.040038
-0.470511	55.175150	0.045043
-0.505967	44.357346	0.050048
-0.821772	34.445644	0.055053
-1.380536	29.709008	0.060058
-1.661969	18.884517	0.065062
-2.241067	26.573480	0.070067
-2.226213	8.441020	0.075072
-2.359392	1.310186	0.080077
-2.661504	6.152107	0.085082
-2.827849	3.545566	0.090086
-3.378896	4.394891	0.095091
-3.570669	-5.570528	0.100096
-4.356310	-11.412950	0.105101
-4.815618	-7.258219	0.110106
-5.034174	-11.494955	0.115110
-5.088226	5.545183	0.120115
-4.993339	-5.782755	0.125120
-4.897480	-6.112499	0.130125
-5.146962	-2.982821	0.135130
-5.389858	-9.991439	0.140134
-6.522124	3.817229	0.145139
-6.334468	-5.934762	0.150144
-6.298389	-13.538683	0.155149
-6.776520	2.835680	0.160154
-6.309581	-3.663206	0.165158
-7.533922	-5.425048	0.170163
-7.749723	-9.353949	0.175168
-7.990685	-12.890786	0.180173
-8.208502	0.784913	0.185178
-8.127228	-5.429058	0.190182
-8.336192	-5.325258	0.195187
-8.911846	2.615577	0.200192
-9.131696	-3.010379	0.205197
-9.884223	1.767367	0.210202
-9.322036	3.786837	0.215206
-10.153335	0.013120	0.220211
-9.612418	-4.114233	0.225216
-9.441214	-7.808762	0.230221
-10.977369	6.134626	0.235226
-11.187473	5.572309	0.240230
-11.420996	-1.556146	0.245235
-11.239792	-3.457728	0.250240
-11.164951	-7.280366	0.255245
-11.751294	-0.236693	0.260250
-11.655475	-4.828051	0.265254
-12.572523	-2.726116	0.270259
-12.588375	-3.431814	0.275264
-12.781198	-1.717406	0.280269
-12.975493	5.584767	0.285274
-12.941465	-7.545273	0.290278
-13.955075	7.536541	0.295283
-14.317972	5.863483	0.300288
-14.091790	2.796377	0.305293
-14.767714	-5.977012	0.310298
-14.380621	-0.086953	0.315302
-14.832747	3.299466	0.320307
-14.501267	5.838983	0.325312
-14.882348	-3.611750	0.330317
-15.921534	5.474005	0.335322
-15.597407	3.484579	0.340326
-15.989173	6.069234	0.345331
-16.218158	6.625905	0.350336
-16.816182	7.733475	0.355341
-17.425736	5.209157	0.360346
-17.363562	-0.846477	0.365350
-17.794803	3.201315	0.370355
-17.442928	7.764687	0.375360
-17.709364	11.989754	0.380365
-18.064332	2.473044	0.385370
-17.540841	-7.263612	0.390374
-18.510643	13.265896	0.395379
-19.109176	6.684120	0.400384
-19.108015	3.542920	0.405389
-19.476815	22.021561	0.410394
-19.136086	0.463683	0.415398
-19.369793	6.421018	0.420403
-20.003495	7.406531	0.425408
-20.345357	1.061233	0.430413
-20.621398	10.892970	0.435418
-20.820056	9.632566	0.440422
-20.950120	7.237561	0.445427
-21.622307	8.349988	0.450432
-21.759113	4.661471	0.455437
-22.542278	10.863016	0.460442
-22.276067	5.320891	0.465446
-22.466136	10.073661	0.470451
-22.255286	9.437241	0.475456
-22.109598	8.733061	0.480461
-23.243317	3.487794	0.485466
-23.517020	-6.361779	0.490470
-23.747535	3.721985	0.495475
-23.895087	0.330021	0.500480
-24.165657	4.918715	0.505485
-24.353296	5.033295	0.510490
-24.378721	-4.987531	0.515494
-24.178550	5.758250	0.520499
-24.791219	2.079810	0.525504
-25.295774	-0.742823	0.530509
-25.718485	9.595566	0.535514
-25.705806	-1.245351	0.540518
-26.629105	2.448797	0.545523
-27.096859	10.699729	0.550528
-26.582208	4.722723	0.555533
-27.071097	2.471662	0.560538
-27.256844	-5.391167	0.565542
-27.672153	3.331929	0.570547
-27.347699	-0.625879	0.575552
-27.664621	-2.532152	0.580557
-27.796262	-3.489716	0.585562
-27.981324	2.959060	0.590566
-28.789910	11.910228	0.595571
-29.512971	-0.968521	0.600576
-29.464227	5.802786	0.605581
-29.662438	8.197707	0.610586
-29.524201	3.745048	0.615590
-29.710382	5.816372	0.620595
-29.530932	0.947886	0.625600
-30.156710	-7.777652	0.630605
-30.801974	7.271405	0.635610
-30.854872	9.144607	0.640614
-30.628301	4.175599	0.645619
-31.313703	8.744061	0.650624
-31.807605	13.469897	0.655629
-32.630041	8.903813	0.660634
-32.398535	7.963777	0.665638
-32.379303	9.574874	0.670643
-32.265035	9.464551	0.675648
-32.303599	7.523422	0.680653
-32.873117	8.848253	0.685658
-33.428722	9.876205	0.690662
-33.846834	8.481103	0.695667
-33.961110	6.159058	0.700672
-33.898347	4.157086	0.705677
-34.163294	16.875658	0.710682
-34.326184	0.929049	0.715686
-35.342124	8.543598	0.720691
-35.662612	0.552391	0.725696
-35.378792	-8.681183	0.730701
-35.739845	3.867003	0.735706
-35.461261	0.009016	0.740710
-35.706498	-10.419419	0.745715
-36.166888	-1.460395	0.750720
-36.174824	0.390479	0.755725
-36.908534	-2.379977	0.760730
-36.712562	-4.480221	0.765734
-37.689889	0.920678	0.770739
-38.199853	4.433363	0.775744
-38.156559	-1.962067	0.780749
-38.164901	0.823415	0.785754
-38.093920	1.073818	0.790758
-38.235522	2.753323	0.795763
-38.618703	4.079323	0.800768
-39.623858	-4.289335	0.805773
-40.240109	-5.652479	0.810778
-39.396749	-7.795981	0.815782
-39.630539	-7.744803	0.820787
-40.509475	-11.048845	0.825792
-40.132785	-3.711705	0.830797
-40.592309	4.912647	0.835802
-40.402569	-6.933403	0.840806
-41.378410	2.002388	0.845811
-41.052739	-5.436697	0.850816
-41.640635	-4.676578	0.855821
-41.678094	7.057812	0.860826
-41.893418	-11.912914	0.865830
-42.959311	-4.951387	0.870835
-43.317288	-2.154885	0.875840
-42.864233	-15.263897	0.880845
-43.261941	2.014053	0.885850
-43.164669	-11.677705	0.890854
-43.275165	-2.453121	0.895859
-43.737822	2.618753	0.900864
-43.964407	-6.639877	0.905869
-44.626540	8.790303	0.910874
-45.003595	7.889575	0.915878
-45.084202	4.438306	0.920883
-45.281140	7.808303	0.925888
-45.213422	-0.429074	0.930893
-45.265833	0.712632	0.935898
-45.478346	4.983637	0.940902
-46.445739	-1.075870	0.945907
-46.549551	9.533299	0.950912
-46.631904	-1.501745	0.955917
-46.949568	7.360693	0.960922
-46.913835	5.385385	0.965926
-47.619647	-3.138497	0.970931
-47.949748	-4.521111	0.975936
-47.956538	0.707162	0.980941
-48.238168	-0.585401	0.985946
-48.247106	4.380810	0.990950
-48.245332	4.626570	0.995955
-48.638689	-7.046856	1.000960
-49.089318	-0.676129	1.005965
-49.755318	-4.932342	1.010970
-49.770820	-12.397316	1.015974
-49.838864	-5.150247	1.020979
-49.875808	-6.342371	1.025984
-49.608562	-12.875828	1.030989
-50.898949	1.511034	1.035994
-51.164746	-9.698787	1.040998
-51.546543	-1.154862	1.046003
-51.405611	-7.798458	1.051008
-51.543304	-1.155077	1.056013
-51.917731	9.969587	1.061018
-52.291040	-1.377949	1.066022
-52.852545	-1.224271	1.071027
-53.036540	-8.499314	1.076032
-53.191757	-12.385641	1.081037
-53.267539	-9.075427	1.086042
-53.417604	-4.463737	1.091046
-53.304220	-6.772104	1.096051
-53.653191	9.264634	1.101056
-53.643032	-8.309828	1.106061
-54.386507	-1.923557	1.111066
-54.628149	-4.329517	1.116070
-54.993401	-1.661937	1.121075
-54.830259	0.236232	1.126080
-55.639077	-5.930571	1.131085
-56.159239	-4.786244	1.136090
-56.601950	-7.185413	1.141094
-56.703136	-7.899699	1.146099
-56.015652	-2.877519	1.151104
-56.352304	-1.661611	1.156109
-56.695990	-2.574264	1.161114
-56.757502	-2.022777	1.166118
-57.508052	-5.035402	1.171123
-57.843729	-4.973009	1.176128
-58.314899	-5.802244	1.181133
-58.627216	4.900965	1.186138
-58.316584	-0.899077	1.191142
-57.942659	2.574375	1.196147
-58.595553	-9.658827	1.201152
-59.212654	-10.587163	1.206157
-59.324759	-2.746023	1.211162
-59.516217	-6.056442	1.216166
-59.622393	-3.681467	1.221171
-60.392192	1.071810	1.226176
-60.878032	-10.765086	1.231181
-61.181287	-4.834540	1.236186
-61.130828	-12.183546	1.241190
-61.459449	0.214354	1.246195
-61.442148	-1.008241	1.251200
-61.449296	-13.137337	1.256205
-61.417570	-9.365930	1.261210
-61.939845	-7.229395	1.266214
-62.475320	-8.107787	1.271219
-62.679069	-6.853960	1.276224
-62.560245	-0.152840	1.281229
-63.175902	0.908814	1.286234
-63.625929	1.950199	1.291238
-64.146970	1.586956	1.296243
-64.423124	3.544505	1.301248
-64.277688	-6.741814	1.306253
-64.379273	2.746577	1.311258
-64.268066	1.808171	1.316262
-64.548399	8.179958	1.321267
-65.307997	3.903896	1.326272
-65.601517	-3.944078	1.331277
-66.188059	9.278083	1.336282
-66.191927	-2.704865	1.341286
-66.060739	4.439435	1.346291
-66.249224	-4.003414	1.351296
-66.168867	-8.066787	1.356301
-67.127877	0.842053	1.361306
-67.553290	2.643734	1.366310
-67.746897	1.006236	1.371315
-67.857317	-1.687972	1.376320
-67.944587	2.415439	1.381325
-67.812581	10.555017	1.386330
-67.689475	-5.538089	1.391334
-68.528307	-3.535888	1.396339
-69.261165	3.803298	1.401344
-68.968994	-9.536317	1.406349
-69.382533	0.812386	1.411354
-69.563513	-4.930183	1.416358
-70.537650	-1.519939	1.421363
-70.780131	5.372202	1.426368
-70.769373	-3.200945	1.431373
-71.245694	6.066343	1.436378
-71.292723	9.293674	1.441382
-71.037495	-6.890519	1.446387
-71.301658	4.085892	1.451392
-71.068837	-1.163829	1.456397
-71.506443	-2.607300	1.461402
-72.213483	-2.723062	1.466406
-72.538596	-2.319396	1.471411
-72.963666	1.219905	1.476416
-72.547682	-2.185182	1.481421
-72.814148	-1.140888	1.486426
-73.314302	-9.454288	1.491430
-73.703580	-1.327021	1.496435
-74.404991	-1.007271	1.501440
-74.066445	-5.993696	1.506445
-74.401314	-6.465741	1.511450
-74.530283	-18.446251	1.516454
-75.381678	-8.545389	1.521459
-75.800456	-6.536449	1.526464
-75.841719	-9.165825	1.531469
-76.108383	0.496247	1.536474
-75.910871	-2.085976	1.541478
-75.872551	-2.237119	1.546483
-76.136222	-10.853498	1.551488
-76.098414	-10.865950	1.556493
-76.889106	-9.503775	1.561498
-77.088617	-2.818315	1.566502
-77.279586	-15.468301	1.571507
-77.515989	0.767549	1.576512
-77.943369	-0.164518	1.581517
-78.773636	1.723015	1.586522
-78.840744	-4.895669	1.591526
-79.261013	-12.441232	1.596531
-79.231611	-1.318206	1.601536
-78.801225	-3.874494	1.606541
-79.211790	-5.986961	1.611546
-79.338013	5.685835	1.616550
-80.181688	-4.384236	1.621555
-80.656606	-4.235593	1.626560
-80.810055	-4.049613	1.631565
-80.883861	-12.344980	1.636570
-80.956476	-2.947506	1.641574
-80.912324	-3.305503	1.646579
-81.303852	1.223961	1.651584
-81.519301	1.061189	1.656589
-82.563107	-2.053512	1.661594
-82.764430	-9.553280	1.666598
-82.710284	-1.082489	1.671603
-82.727311	-1.117545	1.676608
-82.475737	-12.429734	1.681613
-82.600312	-2.932320	1.686618
-83.056259	5.559245	1.691622
-83.743939	-2.081722	1.696627
-84.060318	4.299671	1.701632
-84.127067	-4.458761	1.706637
-84.195430	-6.297098	1.711642
-84.737288	-1.870052	1.716646
-85.742755	0.239699	1.721651
-86.138347	0.077398	1.726656
-85.629254	-3.500034	1.731661
-85.843149	7.414304	1.736666
-85.966935	-2.816077	1.741670
-86.030699	1.162795	1.746675
-85.940077	0.389878	1.751680
-86.245135	-6.540684	1.756685
-87.172388	-3.068438	1.761690
-87.433714	6.203074	1.766694
-87.498110	-2.920763	1.771699
-87.589145	-2.046338	1.776704
-87.902944	-14.267501	1.781709
-88.623513	-2.728714	1.786714
-89.237999	-1.700103	1.791718
-89.089402	-10.733551	1.796723
-89.108177	2.108970	1.801728
-88.901108	-14.018323	1.806733
-89.238946	-9.628154	1.811738
-89.374650	1.717394	1.816742
-89.670827	-4.916802	1.821747
-90.393619	-4.700655	1.826752
-90.297364	-2.506721	1.831757
-90.667878	3.775297	1.836762
-90.559892	-7.969632	1.841766
-91.423704	2.010733	1.846771
-91.865207	1.116911	1.851776
-91.924313	-4.832943	1.856781
-92.162667	0.325474	1.861786
-92.090423	-7.444732	1.866790
-91.891807	-7.892973	1.871795
-92.438546	3.966913	1.876800
-92.840751	-5.008951	1.881805
-93.671118	-5.416762	1.886810
-93.736129	0.776092	1.891814
-93.804031	-6.227798	1.896819
-94.009955	-4.818233	1.901824
-94.165024	-8.870023	1.906829
-95.040136	-11.464286	1.911834
-95.471985	-1.402402	1.916838
-95.260108	-0.216870	1.921843
-95.461309	0.431497	1.926848
-95.412094	-5.686114	1.931853
-95.661318	-0.988189	1.936858
-95.649205	-1.387455	1.941862
-95.946990	3.700678	1.946867
-96.557446	4.734642	1.951872
-96.840096	-4.478708	1.956877
-97.261673	0.572764	1.961882
-97.199412	-1.023166	1.966886
-97.039843	-3.041135	1.971891
-97.731100	6.011688	1.976896
-98.344446	-10.298370	1.981901
-98.756993	-7.097743	1.986906
-98.687567	-9.004331	1.991910
-98.820977	-9.431733	1.996915
-99.014671	-1.786366	2.006912
-98.815263	-1.730842	2.016909
-97.747779	3.389904	2.026906
-97.409290	-2.158349	2.036902
-97.614650	-3.542364	2.046899
-97.261815	3.733572	2.056896
-96.435852	0.723593	2.066893
-95.513601	3.351541	2.076890
-94.648694	7.269149	2.086886
-94.599202	2.470633	2.096883
-94.239433	-3.629264	2.106880
-94.338468	-2.592827	2.116877
-93.133080	4.512722	2.126874
-92.728201	0.151295	2.136870
-92.311382	-2.137884	2.146867
-91.554208	0.548116	2.156864
-91.335438	0.721692	2.166861
-91.074738	-5.029932	2.176858
-90.101492	-11.940057	2.186854
-89.740301	0.939932	2.196851
-88.754026	2.463169	2.206848
-88.372085	3.750977	2.216845
-88.414834	-0.174344	2.226842
-88.074913	2.055801	2.236838
-87.265761	-3.578981	2.246835
-86.994262	1.517495	2.256832
-85.879809	-2.328767	2.266829
-85.401469	-2.118769	2.276826
-85.156312	-2.549540	2.286822
-85.084317	-1.116568	2.296819
-84.266687	-7.734123	2.306816
-83.905091	6.792655	2.316813
-82.886226	-3.888708	2.326810
-82.347393	0.368115	2.336806
-82.174406	-11.040236	2.346803
-82.377733	4.628695	2.356800
-81.136163	-3.913065	2.366797
-80.782963	-5.458242	2.376794
-79.864954	-0.275797	2.386790
-79.302983	0.941957	2.396787
-79.149079	-1.390450	2.406784
-79.147152	-1.641496	2.416781
-78.164939	4.207621	2.426778
-77.462446	-1.371206	2.436774
-77.480628	-1.238678	2.446771
-76.867733	1.242544	2.456768
-75.974186	9.276849	2.466765
-76.039435	-0.567525	2.476762
-75.004203	-2.371860	2.486758
-74.433524	0.717461	2.496755
-74.359883	4.465800	2.506752
-73.708904	4.309392	2.516749
-72.712616	-3.757152	2.526746
-72.432778	-1.978574	2.536742
-72.749755	0.881346	2.546739
-72.025351	-2.658195	2.556736
-70.904310	1.264401	2.566733
-70.504265	-4.334229	2.576730
-69.959280	4.102272	2.586726
-69.740375	5.073916	2.596723
-69.594492	-5.256277	2.606720
-68.845011	0.918802	2.616717
-68.185280	0.335208	2.626714
-67.355093	1.379828	2.636710
-66.453221	-0.882881	2.646707
-66.888479	3.220415	2.656704
-66.442553	7.494226	2.666701
-65.712356	-4.142337	2.676698
-65.159594	1.496827	2.686694
-64.837715	-0.232337	2.696691
-63.877603	6.262751	2.706688
-63.761778	2.114452	2.716685
-63.338525	4.905279	2.726682
-62.065630	4.483599	2.736678
-62.037142	3.035795	2.746675
-61.932192	0.322683	2.756672
-61.689482	10.051543	2.766669
-60.800048	2.034513	2.776666
-59.584469	-8.499774	2.786662
-59.577633	-0.505622	2.796659
-59.024987	0.857695	2.806656
-58.842365	-0.628916	2.816653
-57.979919	1.538830	2.826650
-57.180349	-1.364298	2.836646
-57.195790	0.533213	2.846643
-57.176775	-0.162992	2.856640
-56.296337	-0.435405	2.866637
-55.879058	3.113901	2.876634
-54.594372	4.273955	2.886630
-54.239067	-5.978684	2.896627
-54.232122	-3.910379	2.906624
-54.012616	0.021834	2.916621
-53.495581	4.635302	2.926618
-52.596035	3.126716	2.936614
-51.553032	-7.354850	2.946611
-51.534845	1.527233	2.956608
-51.090378	6.311977	2.966605
-50.488664	3.632734	2.976602
-50.508124	5.857624	2.986598
-49.760717	-0.062550	2.996595
-49.290089	3.183182	3.006592
-47.967248	1.504677	3.016589
-47.874171	4.150636	3.026586
-47.783331	4.103939	3.036582
-47.396292	0.206367	3.046579
-46.520893	5.404061	3.056576
-45.973033	5.119639	3.066573
-45.965747	4.752135	3.076570
-44.717069	-0.396190	3.086566
-44.484844	0.769183	3.096563
-44.441068	7.053141	3.106560
-43.531999	7.353117	3.116557
-42.885931	4.894380	3.126554
-42.611507	4.226197	3.136550
-42.005445	2.365860	3.146547
-41.261359	3.934958	3.156544
-40.959302	-0.023790	3.166541
-40.986546	10.791563	3.176538
-40.331820	2.911510	3.186534
-39.987605	2.942611	3.196531
-38.936348	4.078669	3.206528
-38.328621	6.438955	3.216525
-38.136920	2.433645	3.226522
-37.996715	3.146504	3.236518
-36.949285	0.816527	3.246515
-36.581825	2.452412	3.256512
-36.061537	4.938424	3.266509
-35.373092	8.740493	3.276506
-35.071991	8.486826	3.286502
-34.754880	-7.541710	3.296499
-33.720767	-8.390509	3.306496
-33.703786	1.042076	3.316493
-33.387550	-7.574097	3.326490
-32.307382	-8.883953	3.336486
-32.131632	-1.996682	3.346483
-31.675916	2.147742	3.356480
-30.529568	1.744018	3.366477
-30.262463	-0.930402	3.376474
-30.153343	-3.529470	3.386470
-29.926946	-3.427878	3.396467
-28.920868	-5.134042	3.406464
-28.698788	0.069483	3.416461
-28.378566	1.275730	3.426458
-26.915500	-7.090548	3.436454
-26.678396	-4.798068	3.446451
-26.675682	-0.959032	3.456448
-26.460846	-6.542907	3.466445
-25.577792	5.626964	3.476442
-24.868968	3.266514	3.486438
-24.612010	-3.229193	3.496435
-23.596475	3.354831	3.506432
-23.436137	-0.488632	3.516429
-23.307735	5.639692	3.526426
-22.892351	1.778824	3.536422
-21.908752	-4.702182	3.546419
-21.581780	3.262629	3.556416
-21.028515	-0.446876	3.566413
-20.463322	-1.577638	3.576410
-20.183786	-3.853807	3.586406
-19.223774	5.096521	3.596403
-18.802213	-3.306954	3.606400
-18.599635	-6.151179	3.616397
-18.469423	0.281431	3.626394
-17.349627	-3.779314	3.636390
-17.165121	-5.492836	3.646387
-16.379254	-3.192313	3.656384
-15.631962	-2.631243	3.666381
-15.556169	-12.509000	3.676378
-15.346545	-2.972380	3.686374
-14.757690	-1.666260	3.696371
-13.790618	-6.088734	3.706368
-13.698572	-3.453371	3.716365
-12.960770	2.701275	3.726362
-12.210616	-8.093871	3.736358
-12.402523	-2.004875	3.746355
-11.528099	-1.299705	3.756352
-10.838083	4.434482	3.766349
-10.691440	3.750573	3.776346
-9.745894	1.242397	3.786342
-8.983021	4.014888	3.796339
-8.948401	0.173235	3.806336
-8.826623	9.790859	3.816333
-8.262682	2.294800	3.826330
-7.538392	5.104635	3.836326
-7.042503	-3.332262	3.846323
-6.122128	-1.770956	3.856320
-5.583924	-0.835333	3.866317
-5.603818	3.800147	3.876314
-5.289663	-0.625211	3.886310
-4.547283	5.692656	3.896307
-4.348358	6.006325	3.906304
-3.967051	13.823774	3.916301
-3.624091	30.436342	3.926298
-2.626897	45.307092	3.936294
-2.146887	47.983106	3.946291
-2.021548	65.500839	3.956288
-1.514456	84.618814	3.966285
-1.097452	91.350343	3.976282
-0.419777	111.204423	3.986278
0.000000	126.877034	3.991283
0.395912	136.724184	3.996288
0.354580	143.282154	4.001293
0.603416	143.333384	4.006298
0.223853	144.481909	4.011302
0.257609	131.285992	4.016307
0.877331	156.024312	4.021312
0.914826	172.339197	4.026317
0.994242	160.472376	4.031322
0.784700	154.399628	4.036326
0.622518	141.485184	4.041331
0.799332	145.933395	4.046336
0.857207	150.555460	4.051341
1.210908	154.969707	4.056346
0.960299	147.482338	4.061350
1.024855	140.543595	4.066355
0.875566	137.192827	4.071360
0.605331	144.414092	4.076365
0.900892	137.626197	4.081370
0.994680	146.514839	4.086374
0.891493	144.304785	4.091379
0.850939	144.567309	4.096384
0.761339	142.396445	4.101389
1.223394	137.250067	4.106394
0.911410	145.369868	4.111398
0.968812	143.514081	4.116403
1.335695	130.673219	4.121408
0.967563	141.202155	4.126413
0.687742	133.686374	4.131418
0.790143	147.752341	4.136422
1.357431	166.077155	4.141427
1.349667	147.838070	4.146432
1.014701	143.449265	4.151437
0.930317	134.974823	4.156442
1.206156	138.562288	4.161446
0.973810	133.303267	4.166451
0.992174	149.665190	4.171456
1.365955	157.391690	4.176461
1.162424	139.811619	4.181466
1.108425	152.611955	4.186470
1.222652	148.121491	4.191475
1.292590	153.813835	4.196480
1.136814	143.982063	4.201485
1.077142	132.760658	4.206490
1.571065	149.043105	4.211494
0.816338	148.451511	4.216499
1.139960	149.032981	4.221504
1.394911	166.362098	4.226509
1.659235	161.177061	4.231514
1.335227	151.536852	4.236518
1.107131	149.112150	4.241523
1.365627	151.637314	4.246528
1.072819	157.723254	4.251533
1.769464	157.691603	4.256538
1.445336	155.108152	4.261542
1.135831	145.721163	4.266547
1.265652	150.538906	4.271552
1.374143	160.655443	4.276557
1.634783	163.129645	4.281562
1.210367	154.367674	4.286566
1.375383	162.143079	4.291571
1.708424	168.121159	4.296576
1.417826	157.905499	4.301581
1.283543	146.048749	4.306586
0.973755	148.920675	4.311590
1.332751	163.059481	4.316595
1.794228	166.147568	4.321600
1.449262	177.070080	4.326605
1.831433	167.128283	4.331610
1.589731	181.960570	4.336614
1.730267	174.543113	4.341619
1.870898	164.741663	4.346624
1.364308	157.209776	4.351629
1.623534	158.148658	4.356634
1.531226	169.673525	4.361638
1.540780	164.367514	4.366643
2.085556	167.878085	4.371648
1.566521	165.451047	4.376653
1.530791	140.178498	4.381658
1.376462	154.375884	4.386662
1.096106	167.816911	4.391667
1.859167	156.854637	4.396672
1.199096	175.771284	4.401677
1.700461	165.429084	4.406682
1.606305	168.561342	4.411686
1.601207	172.823768	4.416691
1.682270	172.692689	4.421696
1.479324	177.570859	4.426701
1.634898	169.592042	4.431706
1.371616	180.666403	4.436710
1.313772	180.904655	4.441715
2.226527	190.325183	4.446720
2.086980	202.752776	4.451725
2.240604	175.505383	4.456730
1.942165	171.732253	4.461734
1.911675	178.812202	4.466739
1.746437	171.324722	4.471744
1.447864	181.826703	4.476749
1.549463	179.680667	4.481754
1.713008	192.563571	4.486758
1.687210	198.769366	4.491763
2.226636	201.593897	4.496768
1.920567	205.224268	4.501773
1.988937	202.259757	4.506778
2.486729	207.088826	4.511782
2.057707	198.906495	4.516787
1.860317	182.893374	4.521792
1.925482	190.702658	4.526797
2.231420	196.495022	4.531802
1.982485	192.226155	4.536806
2.176192	195.224822	4.541811
2.007752	190.510152	4.546816
2.009615	197.497059	4.551821
1.842853	194.077741	4.556826
2.274586	210.733677	4.561830
2.193118	202.317317	4.566835
1.934082	191.925845	4.571840
2.299602	213.451854	4.576845
2.000756	207.418210	4.581850
1.803761	215.429368	4.586854
2.186057	209.138337	4.591859
2.421468	208.267492	4.596864
2.364242	217.643426	4.601869
2.177097	199.697726	4.606874
2.146986	210.039935	4.611878
2.142166	217.399587	4.616883
2.741142	207.066188	4.621888
2.302323	212.926288	4.626893
1.964227	210.561287	4.631898
2.168616	209.685408	4.636902
2.195332	211.313935	4.641907
2.751541	223.888102	4.646912
2.368944	206.920988	4.651917
2.453748	209.757215	4.656922
2.163179	214.046209	4.661926
2.159156	209.005735	4.666931
2.285498	206.944790	4.671936
2.111939	207.588793	4.676941
2.290204	209.680517	4.681946
2.228343	206.091636	4.686950
2.411279	212.138046	4.691955
2.458595	220.129649	4.696960
2.179484	208.336344	4.701965
2.389052	215.284003	4.706970
2.386049	209.657549	4.711974
2.122732	206.233565	4.716979
2.276386	211.877370	4.721984
2.389526	212.872361	4.726989
2.514394	197.215880	4.731994
2.126267	215.010722	4.736998
2.865119	217.231584	4.742003
2.871753	218.268741	4.747008
2.345151	230.501252	4.752013
2.611018	205.230353	4.757018
2.316635	220.894754	4.762022
2.355883	235.673265	4.767027
2.590370	229.807781	4.772032
2.576254	229.187122	4.777037
2.708563	241.590340	4.782042
2.833892	241.225928	4.787046
2.715516	245.557210	4.792051
2.857662	247.214514	4.797056
2.303599	240.614432	4.802061
2.793998	240.336981	4.807066
2.836141	241.454989	4.812070
2.892644	246.399220	4.817075
3.059362	244.722370	4.822080
3.032721	241.653984	4.827085
2.472447	216.642415	4.832090
2.453706	223.188497	4.837094
3.022759	233.251662	4.842099
2.846010	242.404475	4.847104
2.777809	243.463866	4.852109
2.892553	241.869498	4.857114
2.825261	232.758321	4.862118
2.861242	244.491811	4.867123
2.974190	235.544703	4.872128
2.989065	241.204745	4.877133
3.154823	243.699375	4.882138
2.488090	236.886963	4.887142
2.587303	242.834359	4.892147
3.047199	244.165090	4.897152
2.813021	239.119133	4.902157
2.909391	239.621059	4.907162
2.616688	251.779122	4.912166
2.545667	246.399286	4.917171
2.828566	250.167233	4.922176
2.578259	250.053327	4.927181
2.530670	245.466257	4.932186
2.953841	247.597524	4.937190
3.024361	260.883769	4.942195
2.957900	258.988652	4.947200
2.923618	262.059636	4.952205
3.173975	253.576476	4.957210
3.697976	269.065630	4.962214
2.934116	261.830834	4.967219
2.926272	272.812142	4.972224
3.086365	268.221919	4.977229
3.193242	262.237421	4.982234
3.590845	263.617121	4.987238
2.709259	262.554001	4.992243
3.192507	263.519699	4.997248
3.081451	269.232920	5.002253
2.944520	272.097514	5.007258
3.262352	268.667057	5.012262
2.942460	270.054241	5.017267
3.744728	257.900670	5.022272
3.263858	277.585156	5.027277
3.229228	265.034678	5.032282
3.476256	264.154215	5.037286
3.410323	268.653726	5.042291
3.537916	259.902184	5.047296
3.066453	268.372288	5.052301
3.618382	265.849247	5.057306
3.633639	268.531928	5.062310
3.430493	264.914390	5.067315
3.519791	259.022871	5.072320
3.060741	258.600536	5.077325
3.265387	262.614441	5.082330
3.416136	258.750188	5.087334
3.313635	275.324892	5.092339
3.324600	262.284458	5.097344
3.481058	270.398437	5.102349
3.539685	265.248542	5.107354
3.249786	269.479628	5.112358
3.369967	256.288559	5.117363
3.465233	261.341223	5.122368
3.223420	268.503983	5.127373
3.395203	260.910846	5.132378
3.376076	268.841534	5.137382
3.346391	272.462946	5.142387
3.658051	259.997506	5.147392
3.400857	266.320196	5.152397
3.833022	258.343967	5.157402
3.553821	271.947477	5.162406
3.342209	270.444822	5.167411
3.635437	274.554388	5.172416
3.587214	273.644582	5.177421
3.910093	263.847481	5.182426
3.575251	261.822689	5.187430
3.417665	261.607433	5.192435
3.671939	259.981323	5.197440
3.382948	263.474516	5.202445
3.693743	278.861389	5.207450
3.630337	279.850636	5.212454
3.553948	300.671506	5.217459
3.498807	288.659108	5.222464
3.624646	300.313567	5.227469
3.449550	295.129083	5.232474
3.471595	299.517974	5.237478
3.696369	301.976126	5.242483
3.858701	294.635217	5.247488
3.785169	291.939791	5.252493
3.907077	290.843527	5.257498
3.871783	295.446897	5.262502
3.491195	303.574665	5.267507
3.668865	295.058309	5.272512
3.995130	302.836144	5.277517
4.168541	294.056688	5.282522
4.172800	297.254593	5.287526
3.957122	311.984247	5.292531
3.796397	301.973245	5.297536
3.625759	303.784747	5.302541
3.659647	305.898864	5.307546
3.518178	297.251945	5.312550
3.643390	319.289978	5.317555
4.082031	312.696489	5.322560
4.299447	327.903603	5.327565
4.425355	331.459854	5.332570
4.239568	319.288582	5.337574
3.366895	323.582546	5.342579
3.530214	323.698224	5.347584
3.839130	323.224843	5.352589
3.876771	333.243891	5.357594
4.210022	325.800434	5.362598
3.563948	324.454415	5.367603
4.222440	322.926649	5.372608
4.147433	340.374122	5.377613
4.005549	323.081790	5.382618
4.309394	323.417233	5.387622
4.250008	336.223349	5.392627
4.163512	323.430710	5.397632
3.752980	331.197134	5.402637
4.017469	322.250189	5.407642
4.038705	341.135149	5.412646
4.182424	355.120289	5.417651
4.749052	362.788980	5.422656
4.463141	344.026484	5.427661
4.378522	340.861012	5.432666
4.598014	327.979328	5.437670
4.395387	333.647822	5.442675
4.418260	321.432300	5.447680
4.318010	322.922591	5.452685
4.370714	316.354600	5.457690
4.499684	325.344967	5.462694
4.188893	331.648029	5.467699
4.529655	321.938995	5.472704
4.303419	329.800254	5.477709
4.402368	320.320008	5.482714
4.679139	332.417175	5.487718
4.567740	332.092868	5.492723
4.440131	326.109310	5.497728
4.286987	327.635276	5.502733
4.401484	329.294297	5.507738
4.671986	336.820322	5.512742
4.512327	332.068247	5.517747
4.653918	316.979799	5.522752
4.506916	333.663337	5.527757
4.480338	330.817193	5.532762
4.549263	330.212107	5.537766
4.646327	336.539126	5.542771
4.621114	327.469182	5.547776
4.624403	326.698645	5.552781
4.593518	323.503481	5.557786
4.643908	310.048157	5.562790
4.549529	333.662706	5.567795
4.403934	318.475113	5.572800
4.545930	325.957059	5.577805
4.531622	326.425089	5.582810
4.732501	329.275008	5.587814
4.616929	324.239513	5.592819
4.514634	323.712543	5.597824
4.538293	335.888635	5.602829
4.595689	323.971758	5.607834
4.718615	321.652688	5.612838
4.295924	343.203081	5.617843
4.952376	348.607379	5.622848
4.629526	362.947049	5.627853
4.638720	355.788181	5.632858
4.916840	355.929185	5.637862
4.862790	372.002511	5.642867
5.367320	358.320068	5.647872
4.781449	357.531267	5.652877
4.597437	337.712012	5.657882
4.982430	344.930948	5.662886
4.794549	361.513737	5.667891
4.995990	350.080717	5.672896
4.678618	370.670499	5.677901
4.660292	363.636633	5.682906
4.421500	358.224007	5.687910
4.463675	366.329791	5.692915
5.117216	359.197527	5.697920
4.747395	360.920112	5.702925
4.808282	364.659762	5.707930
5.174973	350.522217	5.712934
4.792274	359.925485	5.717939
4.796134	364.685582	5.722944
4.605979	366.806642	5.727949
4.873033	365.166571	5.732954
5.102141	373.052246	5.737958
5.076759	369.992703	5.742963
5.193714	366.489957	5.747968
5.240274	371.629138	5.752973
5.030379	362.245877	5.757978
5.195332	365.485313	5.762982
4.784908	365.569231	5.767987
5.026339	365.817025	5.772992
5.579172	385.918319	5.777997
5.078604	372.442508	5.783002
5.550512	366.136111	5.788006
5.278859	362.542795	5.793011
5.168894	352.529685	5.798016
5.012681	368.779121	5.803021
5.050924	367.013291	5.808026
5.431656	369.018009	5.813030
5.372256	375.769667	5.818035
5.181291	369.202655	5.823040
5.323201	364.503434	5.828045
5.237460	359.680928	5.833050
5.443675	350.767767	5.838054
5.057299	360.624472	5.843059
5.214764	355.702090	5.848064
5.326241	366.093320	5.853069
5.343994	369.472115	5.858074
5.426507	357.552343	5.863078
5.133095	369.660105	5.868083
5.555963	376.577027	5.873088
5.445059	384.614495	5.878093
5.480377	375.450169	5.883098
5.469212	366.520042	5.888102
5.125987	365.838633	5.893107
5.743555	375.638455	5.898112
5.540387	381.964300	5.903117
5.333582	366.299910	5.908122
5.753256	371.342113	5.913126
5.311692	360.084699	5.918131
5.208087	368.256900	5.923136
5.551297	382.183152	5.928141
5.802474	387.493234	5.933146
5.746566	380.797943	5.938150
5.591588	367.994288	5.943155
5.377822	365.594412	5.948160
5.625157	363.133233	5.953165
5.488257	371.065778	5.958170
5.564852	378.506171	5.963174
5.452759	385.948153	5.968179
5.616555	384.225600	5.973184
5.689961	386.264928	5.978189
5.697644	403.300436	5.983194
5.650914	385.098389	5.988198
5.616912	392.541873	5.993203
5.521722	379.969245	5.998208
5.780678	389.961228	6.003213
5.609312	393.192418	6.008218
6.082203	391.314605	6.013222
5.963526	395.299894	6.018227
5.631766	383.963743	6.023232
5.539039	371.336257	6.028237
5.738145	379.910183	6.033242
5.909137	382.155952	6.038246
5.849839	383.155970	6.043251
5.505915	358.749974	6.048256
5.565154	371.061784	6.053261
5.253041	366.893480	6.058266
5.559421	365.470069	6.063270
5.381079	378.951543	6.068275
5.710331	371.654044	6.073280
5.902843	390.860890	6.078285
5.731308	391.149306	6.083290
5.857848	385.434787	6.088294
5.656818	392.519537	6.093299
5.563994	394.428882	6.098304
5.628891	384.737477	6.103309
5.610839	389.440924	6.108314
5.850036	386.518490	6.113318
5.519021	388.763065	6.118323
5.903438	390.302805	6.123328
5.992521	390.655687	6.128333
5.822490	385.467080	6.133338
5.685957	371.417016	6.138342
5.421255	363.848704	6.143347
5.608108	376.597685	6.148352
5.935788	387.353053	6.153357
5.624391	372.823709	6.158362
5.849623	372.193975	6.163366
5.511753	379.389432	6.168371
5.270854	369.331554	6.173376
5.723952	386.889218	6.178381
5.646172	393.987736	6.183386
5.724801	387.632966	6.188390
5.868538	393.438201	6.193395
5.746888	381.303043	6.198400
5.706583	381.986889	6.203405
5.554495	385.269448	6.208410
6.012190	387.068677	6.213414
5.920544	377.120399	6.218419
5.624995	368.640078	6.223424
5.444777	358.421334	6.228429
5.372645	362.398332	6.233434
5.659620	366.711792	6.238438
5.838444	377.076905	6.243443
5.769339	376.945878	6.248448
5.704025	373.950646	6.253453
5.295663	374.586892	6.258458
5.589905	378.762714	6.263462
5.748429	387.906477	6.268467
5.592233	388.778768	6.273472
5.572603	386.757608	6.278477
5.863169	387.070781	6.283482
5.910562	386.632527	6.288486
5.610495	397.788396	6.293491
5.832790	381.462329	6.298496
5.725994	386.634059	6.303501
5.702497	390.152860	6.308506
5.663627	393.459429	6.313510
5.437143	392.900199	6.318515
5.754923	381.880337	6.323520
5.600964	390.236280	6.328525
5.481982	399.162104	6.333530
5.874244	386.096240	6.338534
5.449859	394.859434	6.343539
5.733560	391.982426	6.348544
5.637013	388.662053	6.353549
5.775563	394.170698	6.358554
5.872373	392.569511	6.363558
5.898068	389.349988	6.368563
5.991756	381.126067	6.373568
5.784529	378.091639	6.378573
5.379926	362.639000	6.383578
5.672321	356.342245	6.388582
5.268160	369.641125	6.393587
5.799301	384.075476	6.398592
5.581732	392.553018	6.403597
5.531657	391.092519	6.408602
5.661170	393.984038	6.413606
5.507794	384.668770	6.418611
5.779821	391.964603	6.423616
5.811571	391.243621	6.428621
5.330683	388.562616	6.433626
5.652885	383.152575	6.438630
5.461841	384.060221	6.443635
5.480878	381.975649	6.448640
5.974039	384.720551	6.453645
5.650634	390.305140	6.458650
5.747643	388.881008	6.463654
5.754267	391.691811	6.468659
5.795483	383.824321	6.473664
6.206121	391.685039	6.478669
5.834763	396.373080	6.483674
5.779270	385.372577	6.488678
5.649957	389.484620	6.493683
5.477835	366.519598	6.498688
5.555622	368.316593	6.503693
5.707652	395.293640	6.508698
5.800949	389.580372	6.513702
5.456254	394.325270	6.518707
5.590094	389.222295	6.523712
5.753731	397.014425	6.528717
5.595149	391.268393	6.533722
5.814874	391.306974	6.538726
5.807084	401.087922	6.543731
5.849654	396.124334	6.548736
5.767706	396.905825	6.553741
5.443862	385.727594	6.558746
5.640255	386.740113	6.563750
5.515078	390.340929	6.568755
5.845790	388.507822	6.573760
5.707145	396.366183	6.578765
5.444930	400.697700	6.583770
5.583401	392.415466	6.588774
5.454776	396.763973	6.593779
5.655859	393.389284	6.598784
5.724426	389.169903	6.603789
5.451202	395.152565	6.608794
5.249673	388.762405	6.613798
5.371972	388.033661	6.618803
5.180225	383.452614	6.623808
5.420754	386.506523	6.628813
5.336936	396.995653	6.633818
5.594688	402.736175	6.638822
5.700517	422.964957	6.643827
5.562864	423.244617	6.648832
5.823884	420.834837	6.653837
5.691243	422.474825	6.658842
6.015170	424.367098	6.663846
5.494472	400.456595	6.668851
5.691818	404.982584	6.673856
5.795845	410.193474	6.678861
5.643436	406.288224	6.683866
5.874529	394.059840	6.688870
5.774325	394.840204	6.693875
5.738828	391.596361	6.698880
5.847797	383.404147	6.703885
5.587124	401.708811	6.708890
5.749558	393.734961	6.713894
5.688102	394.487514	6.718899
5.681532	390.747191	6.723904
5.759537	390.456498	6.728909
5.610481	398.098057	6.733914
5.801304	396.518330	6.738918
5.701616	392.199191	6.743923
5.934787	400.327100	6.748928
5.845924	396.076118	6.753933
5.917831	395.590502	6.758938
5.887802	391.097662	6.763942
5.936838	400.642212	6.768947
5.660945	387.962801	6.773952
5.613656	391.233962	6.778957
5.539172	395.256245	6.783962
5.763548	384.251324	6.788966
5.704411	396.039519	6.793971
6.209761	389.591835	6.798976
6.118609	392.966632	6.803981
5.652113	384.627217	6.808986
5.773235	372.891755	6.813990
5.583356	373.633170	6.818995
5.792596	378.046099	6.824000
5.463762	371.390192	6.829005
5.594961	383.239758	6.834010
5.684330	387.155839	6.839014
5.700898	388.970450	6.844019
5.388919	394.991480	6.849024
5.662854	388.844168	6.854029
5.671688	390.704847	6.859034
5.772627	399.634876	6.864038
5.831717	391.386971	6.869043
5.601258	393.174136	6.874048
5.913856	389.524712	6.879053
5.725547	395.722814	6.884058
5.516456	382.402057	6.889062
5.648045	393.341665	6.894067
5.655680	401.016822	6.899072
5.996426	397.890553	6.904077
5.668259	397.259829	6.909082
5.526087	377.363858	6.914086
5.292538	386.551004	6.919091
5.475136	391.515090	6.924096
5.942848	397.803673	6.929101
5.526487	396.808093	6.934106
5.547663	391.001970	6.939110
5.422915	400.029968	6.944115
5.501232	403.102103	6.949120
5.436491	392.683319	6.954125
5.315722	399.519712	6.959130
5.452324	393.269899	6.964134
5.439488	401.740349	6.969139
5.831716	404.876135	6.974144
5.699643	384.389314	6.979149
5.543873	387.813954	6.984154
5.688030	398.578545	6.989158
5.479135	402.389919	6.994163
5.733442	404.235783	6.999168
5.710916	399.247336	7.004173
5.559224	392.497329	7.009178
5.542208	393.230897	7.014182
5.617835	411.572043	7.019187
5.729420	413.007606	7.024192
6.184161	404.412648	7.029197
5.580172	404.367843	7.034202
5.997928	399.525456	7.039206
5.711425	403.241133	7.044211
5.531578	400.135584	7.049216
5.469047	397.560063	7.054221
5.215907	403.972705	7.059226
5.510086	400.088956	7.064230
5.851429	412.367401	7.069235
5.647674	421.502289	7.074240
6.160239	417.233107	7.079245
5.458511	407.944020	7.084250
5.740565	399.247279	7.089254
5.694030	404.094641	7.094259
5.740365	395.025263	7.099264
5.788895	394.303185	7.104269
5.418934	392.558836	7.109274
5.864789	392.948357	7.114278
5.593911	396.335788	7.119283
5.614403	389.487184	7.124288
6.145945	386.366284	7.129293
6.050315	400.201798	7.134298
6.381505	397.645859	7.139302
6.034006	397.362442	7.144307
5.844332	399.872130	7.149312
5.926059	401.936427	7.154317
5.786530	402.658374	7.159322
5.933422	400.325467	7.164326
5.979819	377.252399	7.169331
5.485817	382.288337	7.174336
5.668328	369.157508	7.179341
5.378526	366.041724	7.184346
5.602492	373.404980	7.189350
5.785137	388.851912	7.194355
5.555455	381.786867	7.199360
5.728197	389.853033	7.204365
5.891270	391.144236	7.209370
5.626425	376.756857	7.214374
5.714500	377.356545	7.219379
5.458665	372.341253	7.224384
5.656828	374.830255	7.229389
5.635678	391.901394	7.234394
6.205677	379.119199	7.239398
5.343459	376.033388	7.244403
5.500557	375.345755	7.249408
5.954611	371.786413	7.254413
5.669333	375.246659	7.259418
5.620577	373.064968	7.264422
5.549517	371.100749	7.269427
5.493886	377.417898	7.274432
5.871518	392.114693	7.279437
5.705066	392.378493	7.284442
5.780291	395.499282	7.289446
5.764520	388.430848	7.294451
5.333046	384.112280	7.299456
5.578094	383.517648	7.304461
5.309856	387.062884	7.309466
5.822716	394.177546	7.314470
5.804553	403.204802	7.319475
5.649724	388.575677	7.324480
5.764662	397.402664	7.329485
5.584222	399.032099	7.334490
5.709576	396.712913	7.339494
5.497664	402.057501	7.344499
5.784348	393.381505	7.349504
6.002839	403.764646	7.354509
5.459467	411.971955	7.359514
5.749317	398.979140	7.364518
5.641012	397.961855	7.369523
5.685471	398.292317	7.374528
5.992847	385.606495	7.379533
5.757608	401.350096	7.384538
5.362865	389.506899	7.389542
5.942091	389.285997	7.394547
5.622269	393.279467	7.399552
5.803606	387.204086	7.404557
5.494083	394.140729	7.409562
5.736324	391.882731	7.414566
5.895727	405.450379	7.419571
5.789927	395.841338	7.424576
5.664291	378.393440	7.429581
5.262532	381.176822	7.434586
5.349388	379.307655	7.439590
5.596900	391.287272	7.444595
5.687350	406.037952	7.449600
5.902008	387.051801	7.454605
5.832746	401.549773	7.459610
5.877177	402.241616	7.464614
5.750344	394.600881	7.469619
5.662409	387.984574	7.474624
5.599276	374.008604	7.479629
5.425140	373.922360	7.484634
5.771865	384.442047	7.489638
6.067786	393.750653	7.494643
5.498728	373.079654	7.499648
5.707548	384.684257	7.504653
5.949273	385.607301	7.509658
5.848465	378.189083	7.514662
5.884950	376.049736	7.519667
5.483128	362.938623	7.524672
5.284668	371.725635	7.529677
5.445282	369.067467	7.534682
5.833144	383.134324	7.539686
5.863724	385.784798	7.544691
5.629241	380.397990	7.549696
5.559340	377.635455	7.554701
5.755111	386.467526	7.559706
5.590388	390.985568	7.564710
5.732659	387.499450	7.569715
5.563438	387.480269	7.574720
5.730275	400.017706	7.579725
5.678502	401.608219	7.584730
5.767337	395.140772	7.589734
5.610986	385.056086	7.594739
5.798311	395.011963	7.599744
5.599935	375.209535	7.604749
5.562513	387.675549	7.609754
5.424061	382.609583	7.614758
5.830772	401.535391	7.619763
5.617905	401.130773	7.624768
6.045986	392.795253	7.629773
5.863937	388.548327	7.634778
5.555033	383.993744	7.639782
5.582982	377.678726	7.644787
5.370329	381.908028	7.649792
5.796935	386.199209	7.654797
5.916232	401.212178	7.659802
5.808956	390.323029	7.664806
5.436206	374.576743	7.669811
5.665947	380.065775	7.674816
5.962696	388.599202	7.679821
5.717075	391.772025	7.684826
5.371715	377.698160	7.689830
5.759931	386.432033	7.694835
5.259229	395.544748	7.699840
5.937970	399.159811	7.704845
5.371483	404.335988	7.709850
5.631504	401.200466	7.714854
5.869500	394.662494	7.719859
5.896635	397.735688	7.724864
5.931731	396.101192	7.729869
5.298379	388.423607	7.734874
5.835951	383.518509	7.739878
5.872118	398.809611	7.744883
5.659390	387.642515	7.749888
5.543915	364.391603	7.754893
5.663802	389.863833	7.759898
6.002016	390.094351	7.764902
5.387036	378.884523	7.769907
5.526878	391.228412	7.774912
5.882628	400.706195	7.779917
5.543768	395.010277	7.784922
5.927312	393.555268	7.789926
5.743456	375.737170	7.794931
5.277124	374.666979	7.799936
5.892726	383.767959	7.804941
5.666094	389.509795	7.809946
5.707577	377.237879	7.814950
5.742310	379.512084	7.819955
5.348317	382.202235	7.824960
5.649448	382.655529	7.829965
5.561838	407.366025	7.834970
5.618854	399.061534	7.839974
5.800474	396.555371	7.844979
5.939076	403.904928	7.849984
5.911582	390.774650	7.854989
5.522885	376.804827	7.859994
5.476944	383.310881	7.864998
5.892783	393.363462	7.870003
5.775714	401.787997	7.875008
5.705598	373.928861	7.880013
5.568864	377.133113	7.885018
5.629753	369.197465	7.890022
5.614676	372.589578	7.895027
5.616234	382.757870	7.900032
5.727084	386.744788	7.905037
5.786555	395.986908	7.910042
5.501037	381.743327	7.915046
5.525971	395.825580	7.920051
5.338882	394.899351	7.925056
5.719487	394.697263	7.930061
5.263023	399.301600	7.935066
5.598773	401.187280	7.940070
5.732371	389.415706	7.945075
5.753495	399.196808	7.950080
5.700646	392.665465	7.955085
5.690287	400.581552	7.960090
5.460306	395.248650	7.965094
5.611253	403.879975	7.970099
5.728756	403.383272	7.975104
5.882762	400.503030	7.980109
5.660405	398.008872	7.985114
5.734229	387.104004	7.990118
5.983212	396.133604	7.995136
5.556160	403.703272	8.000154
5.890433	396.801085	8.005171
5.835607	398.274805	8.010189
5.878632	398.695273	8.015206
5.634611	397.680129	8.020224
5.799807	403.738056	8.025242
5.765564	397.469775	8.030259
5.679635	395.831291	8.035277
5.825825	392.728474	8.040294
6.150554	395.502957	8.045312
5.797197	382.160306	8.050330
5.504330	371.424132	8.055347
5.684756	382.157657	8.060365
5.686534	386.541571	8.065382
5.719965	389.058450	8.070400
5.727749	407.149166	8.075418
5.700033	389.875570	8.080435
5.447560	402.623735	8.085453
5.729121	401.745408	8.090470
5.827249	399.534891	8.095488
5.367991	407.260245	8.100506
5.786102	398.366082	8.105523
5.741398	392.158968	8.110541
5.682602	400.126735	8.115558
6.141052	394.706561	8.120576
5.780524	395.259846	8.125594
6.051138	394.701174	8.130611
6.112836	394.899017	8.135629
5.736902	394.872296	8.140646
5.767131	402.878687	8.145664
5.430964	407.828581	8.150682
5.828248	405.612711	8.155699
6.039390	407.445247	8.160717
5.892292	398.807051	8.165734
5.880329	397.058432	8.170752
5.760060	405.026913	8.175770
6.128985	410.532487	8.180787
6.223958	405.289280	8.185805
6.034091	403.080104	8.190822
5.916147	395.883338	8.195840
5.503503	399.645633	8.200858
5.864534	400.524660	8.205875
5.761541	391.567140	8.210893
5.666760	398.716719	8.215910
5.869541	394.078992	8.220928
5.812655	395.961429	8.225946
5.651073	399.541418	8.230963
5.656106	395.644681	8.235981
5.495591	402.871548	8.240998
5.783309	402.233884	8.246016
5.620149	400.070876	8.251034
5.671979	411.073060	8.256051
6.044360	428.247729	8.261069
5.898244	427.212565	8.266086
6.000919	436.295945	8.271104
6.057885	437.762117	8.276122
6.197007	431.174683	8.281139
6.257850	426.926171	8.286157
5.717832	413.954522	8.291174
6.165663	408.994464	8.296192
5.788950	406.478541	8.301210
5.948608	413.112952	8.306227
6.144541	440.701984	8.311245
6.025183	418.901056	8.316262
6.065091	411.922435	8.321280
5.680037	410.084517	8.326298
5.902156	422.238730	8.331315
6.231398	429.976675	8.336333
5.946776	436.093106	8.341350
6.181792	431.736692	8.346368
6.125271	438.489892	8.351386
6.111965	431.119157	8.356403
6.356409	423.801973	8.361421
5.951569	416.057754	8.366438
5.895875	398.273134	8.371456
5.696209	419.206011	8.376474
5.799069	422.585547	8.381491
6.183180	428.685242	8.386509
5.742403	432.967832	8.391526
5.841085	426.570608	8.396544
6.275200	439.681618	8.401562
6.398890	429.043558	8.406579
6.199264	428.384384	8.411597
5.883432	438.727322	8.416614
6.170763	431.817821	8.421632
6.306739	439.886563	8.426650
6.111901	431.973015	8.431667
5.982363	432.773108	8.436685
5.764828	430.860171	8.441702
5.983304	432.744637	8.446720
5.971590	435.244481	8.451738
5.988802	426.928550	8.456755
6.226858	423.867031	8.461773
6.160139	429.006999	8.466790
6.376991	421.391979	8.471808
6.272254	434.373772	8.476826
6.036031	426.966075	8.481843
6.493698	427.677592	8.486861
6.373752	429.732919	8.491878
6.407103	427.427810	8.496896
6.081419	435.471485	8.501914
6.170243	432.049076	8.506931
6.209929	430.352239	8.511949
6.132043	435.664000	8.516966
6.322674	425.832128	8.521984
6.388095	433.946180	8.527002
6.130392	419.051204	8.532019
6.438422	437.558972	8.537037
6.179584	431.719049	8.542054
6.387875	435.640101	8.547072
6.109226	432.067441	8.552090
6.625226	430.199784	8.557107
6.276812	439.828772	8.562125
6.506725	435.869278	8.567143
6.584705	430.694899	8.572160
6.204129	422.867452	8.577178
6.374983	428.647347	8.582195
6.616946	438.485595	8.587213
6.140521	433.462762	8.592231
6.322471	425.461071	8.597248
6.327392	429.708089	8.602266
5.912584	435.791518	8.607283
6.163508	431.254855	8.612301
6.323374	435.341652	8.617319
6.445795	423.757057	8.622336
6.243229	432.654510	8.627354
6.373884	430.763642	8.632371
6.583905	422.811732	8.637389
6.453542	429.009239	8.642407
6.439345	426.976695	8.647424
6.156976	427.603956	8.652442
6.012500	423.766657	8.657459
5.783042	433.220897	8.662477
6.062146	432.397195	8.667495
6.305973	426.812126	8.672512
6.233719	443.527529	8.677530
6.325127	449.267619	8.682547
6.690244	458.312365	8.687565
6.196640	453.161584	8.692583
6.388581	445.491430	8.697600
6.551975	458.587463	8.702618
6.217354	458.800614	8.707635
6.768712	456.152176	8.712653
6.206465	457.559196	8.717671
6.565146	460.884952	8.722688
6.624871	448.601596	8.727706
6.432811	456.733511	8.732723
6.758844	448.282694	8.737741
6.479765	434.515112	8.742759
6.587740	439.555462	8.747776
6.287976	421.564646	8.752794
6.386127	432.238098	8.757811
6.405353	446.550409	8.762829
6.029392	459.801111	8.767847
6.405367	459.249528	8.772864
6.432335	459.278837	8.777882
6.553479	459.516748	8.782899
6.790728	457.041649	8.787917
6.687821	462.945029	8.792935
6.486215	468.953679	8.797952
6.512209	457.220560	8.802970
6.822062	462.760515	8.807987
6.888387	449.887412	8.813005
6.731744	462.089488	8.818023
6.740898	452.906553	8.823040
6.480370	430.808926	8.828058
6.195087	435.373235	8.833075
6.707395	428.573377	8.838093
6.719283	450.493854	8.843111
6.678621	458.417522	8.848128
6.925197	445.159592	8.853146
6.514013	434.266093	8.858163
6.583081	437.969653	8.863181
6.339722	443.127009	8.868199
6.638613	450.602221	8.873216
6.974354	445.464556	8.878234
6.347257	452.308510	8.883251
6.454811	453.200990	8.888269
6.495039	464.238686	8.893287
6.839031	449.950004	8.898304
7.045757	457.518288	8.903322
6.727814	458.776199	8.908339
7.095266	453.280018	8.913357
6.550556	441.352111	8.918375
6.213466	430.314410	8.923392
6.660685	444.306045	8.928410
6.479218	459.672282	8.933427
6.682081	458.738566	8.938445
6.642716	468.205499	8.943463
6.715303	465.462003	8.948480
6.817667	456.675781	8.953498
6.992932	465.341361	8.958515
7.137636	454.763380	8.963533
6.598127	460.791654	8.968551
6.701785	468.705451	8.973568
6.990818	461.133098	8.978586
6.835108	467.457126	8.983603
6.697575	469.205883	8.988621
6.649639	456.571787	8.993639
6.909523	462.064893	8.998656
7.065188	463.587380	9.003674
6.663996	447.919897	9.008691
6.735685	443.187701	9.013709
6.659443	463.872140	9.018727
6.784229	458.592597	9.023744
6.927746	454.757195	9.028762
6.586764	458.386918	9.033779
7.134043	452.350793	9.038797
6.819289	460.738960	9.043815
7.062951	459.870633	9.048832
7.008344	455.589135	9.053850
6.699239	455.099496	9.058867
6.864996	446.114457	9.063885
6.881830	454.959626	9.068903
6.891017	456.729893	9.073920
6.689792	455.621667	9.078938
6.815884	458.729908	9.083955
6.931292	457.612458	9.088973
6.972367	462.103064	9.093991
6.997946	454.986763	9.099008
6.920238	449.344018	9.104026
6.835148	460.309231	9.109043
7.015198	450.242429	9.114061
7.182312	459.935712	9.119079
7.041883	458.257813	9.124096
6.929808	438.817656	9.129114
6.533806	439.848259	9.134131
6.709576	448.546614	9.139149
6.756790	451.871586	9.144167
6.916753	455.333701	9.149184
7.128492	454.350104	9.154202
6.878126	454.651475	9.159219
7.179171	459.024529	9.164237
6.546431	454.798618	9.169255
6.712105	452.160090	9.174272
6.897707	455.211262	9.179290
6.890513	469.203028	9.184307
7.164877	463.442955	9.189325
7.111650	461.536516	9.194343
6.795104	462.272653	9.199360
6.859148	467.527906	9.204378
7.111097	470.371997	9.209395
7.085339	462.093456	9.214413
6.830163	458.359660	9.219431
7.064278	452.818304	9.224448
7.234474	458.957593	9.229466
6.948867	461.619215	9.234483
6.813341	460.806366	9.239501
7.198158	471.103506	9.244519
7.083385	477.282023	9.249536
6.895554	465.450009	9.254554
7.158831	474.255546	9.259571
7.198192	484.055272	9.264589
7.332308	495.579536	9.269607
7.349936	485.519281	9.274624
7.198850	462.029498	9.279642
7.403875	466.434559	9.284659
7.289092	462.898676	9.289677
7.108950	455.364399	9.294695
6.648122	463.708414	9.299712
6.854725	465.721788	9.304730
6.951632	479.238189	9.309747
7.194962	500.882549	9.314765
7.354548	491.997892	9.319783
7.033358	508.701759	9.324800
7.251396	490.040178	9.329818
7.334365	497.722419	9.334835
7.332840	492.916694	9.339853
7.219814	500.276084	9.344871
7.026807	496.285205	9.349888
7.263494	495.141609	9.354906
7.524833	495.560642	9.359923
7.404721	493.081515	9.364941
7.382806	498.915630	9.369959
6.993326	479.537107	9.374976
7.530514	489.429730	9.379994
7.048910	483.318789	9.385011
7.554710	488.935799	9.390029
7.186884	490.493923	9.395047
7.303265	499.703690	9.400064
7.354575	495.387358	9.405082
7.112828	500.651432	9.410099
7.100734	498.622763	9.415117
7.760032	499.734928	9.420135
7.247896	510.218697	9.425152
7.786325	489.044937	9.430170
7.229132	480.876448	9.435187
6.970228	476.093581	9.440205
7.395200	477.064584	9.445223
7.305186	500.912893	9.450240
7.704424	496.219544	9.455258
7.427426	486.315041	9.460275
7.171425	474.421663	9.465293
7.326163	481.335304	9.470311
7.103047	498.083077	9.475328
7.594915	493.230652	9.480346
7.387648	500.159547	9.485363
7.282177	494.636900	9.490381
7.610080	489.256373	9.495399
7.397720	498.159221	9.500416
7.794225	503.509810	9.505434
7.601584	496.092417	9.510451
7.125429	483.957616	9.515469
7.418883	489.145346	9.520487
7.321373	496.600476	9.525504
7.378392	495.594422	9.530522
7.507618	493.635687	9.535539
7.524069	498.914069	9.540557
7.548506	493.846233	9.545575
7.419258	499.948133	9.550592
7.786782	497.214343	9.555610
7.608315	486.503958	9.560627
7.456649	494.035246	9.565645
7.542882	489.435054	9.570663
7.409609	494.777735	9.575680
7.397003	495.118737	9.580698
7.727374	493.335084	9.585715
7.620352	499.252935	9.590733
7.983189	499.315501	9.595751
7.520521	503.905306	9.600768
7.572788	493.353300	9.605786
7.621742	502.175180	9.610803
7.512396	492.955025	9.615821
7.865301	493.392186	9.620839
7.720285	484.628328	9.625856
7.547700	464.686926	9.630874
7.429313	471.236334	9.635891
7.335468	486.694396	9.640909
7.700797	488.085013	9.645927
7.259573	500.853725	9.650944
7.721733	494.124612	9.655962
7.200021	492.642761	9.660979
6.943000	497.606370	9.665997
7.316641	496.128986	9.671015
7.804345	507.953020	9.676032
7.699269	494.175720	9.681050
7.680222	493.590223	9.686067
7.419867	499.776767	9.691085
7.455803	487.334354	9.696103
7.508301	513.752292	9.701120
7.225420	517.387189	9.706138
7.428462	524.159331	9.711155
7.845118	533.744113	9.716173
8.277585	521.927733	9.721191
7.957693	524.700718	9.726208
7.975930	531.418676	9.731226
7.737917	524.486622	9.736243
7.996233	532.357082	9.741261
7.997654	518.783179	9.746279
7.497009	499.894163	9.751296
7.386622	504.370745	9.756314
7.825021	519.608037	9.761331
7.525167	526.629984	9.766349
7.709157	521.598949	9.771367
7.666875	522.408047	9.776384
7.767363	529.701267	9.781402
7.713900	523.528120	9.786419
7.902291	522.993462	9.791437
7.958276	523.874000	9.796455
7.561833	526.366783	9.801472
7.768885	521.481413	9.806490
7.985762	528.024251	9.811507
7.941817	521.622904	9.816525
7.915158	513.752571	9.821543
7.876357	528.264763	9.826560
7.814025	527.714070	9.831578
8.063574	516.491782	9.836595
7.991932	525.900515	9.841613
8.224677	528.338328	9.846631
8.044046	525.849319	9.851648
8.132778	527.032355	9.856666
8.273923	521.847016	9.861683
7.655247	520.231413	9.866701
8.090257	520.509564	9.871719
8.128158	524.706286	9.876736
8.182801	514.064325	9.881754
8.083317	512.547630	9.886771
7.879397	512.489529	9.891789
8.179342	509.440398	9.896807
7.638661	513.253400	9.901824
7.883007	517.410690	9.906842
7.992293	512.969344	9.911859
8.069281	531.946912	9.916877
8.208208	516.885332	9.921895
8.065005	519.090548	9.926912
8.206632	529.124139	9.931930
8.279935	516.046326	9.936947
7.527581	516.815417	9.941965
8.022648	523.225388	9.946983
8.168131	524.545964	9.952000
7.729979	519.102887	9.957018
8.079622	524.802692	9.962035
7.807175	529.692302	9.967053
7.977185	518.252004	9.972071
8.037886	526.340414	9.977088
8.239451	526.898826	9.982106
8.236218	517.981920	9.987123
8.015459	537.377323	9.992141
8.141432	525.037693	9.997159
8.109554	528.422888	10.002176
8.139818	522.342280	10.007194
8.260480	527.140160	10.012211
7.845923	530.283834	10.017229
7.939997	523.691899	10.022247
7.864731	520.568677	10.027264
7.913963	526.897437	10.032282
8.225242	524.536446	10.037299
7.913219	538.034962	10.042317
7.935380	542.636372	10.047335
8.257421	545.021840	10.052352
8.074657	554.378004	10.057370
8.383151	546.349336	10.062387
8.208260	557.650849	10.067405
8.344167	550.035759	10.072423
8.610220	551.609487	10.077440
8.643054	550.087258	10.082458
8.642073	531.857113	10.087475
8.343680	539.854116	10.092493
8.345328	520.830307	10.097511
8.325547	525.186334	10.102528
8.238525	533.015556	10.107546
8.689200	524.553842	10.112563
8.384114	531.366758	10.117581
8.022465	524.042523	10.122599
8.454858	529.403820	10.127616
8.065029	524.426674	10.132634
8.442999	519.583222	10.137651
8.139692	521.150171	10.142669
8.286652	520.870832	10.147687
8.354825	526.889439	10.152704
8.161388	528.014008	10.157722
8.288765	517.214484	10.162739
8.270821	538.721895	10.167757
8.283720	536.464235	10.172775
8.497592	538.311491	10.177792
8.711127	563.157845	10.182810
8.500642	529.506324	10.187827
7.903559	536.798018	10.192845
8.685459	538.276953	10.197863
8.462770	551.664478	10.202880
8.589468	552.898907	10.207898
9.143495	548.768524	10.212915
8.634368	534.431808	10.217933
8.649869	531.740736	10.222951
8.485293	527.094203	10.227968
8.241224	522.158408	10.232986
8.575873	526.496210	10.238003
8.722783	519.275987	10.243021
8.385493	515.392985	10.248039
8.437638	518.582834	10.253056
8.209632	522.005260	10.258074
8.355232	524.424212	10.263091
8.441896	532.888179	10.268109
8.235083	542.477101	10.273127
8.708230	554.192674	10.278144
8.439449	559.585816	10.283162
8.828220	549.702917	10.288179
8.660896	550.814217	10.293197
8.472611	553.223600	10.298215
9.014623	553.420500	10.303232
8.715359	556.994543	10.308250
8.403366	551.624779	10.313267
8.694620	548.826140	10.318285
8.529372	562.900399	10.323303
8.477654	553.126307	10.328320
8.573489	565.238228	10.333338
8.739183	556.988714	10.338355
8.958453	552.412571	10.343373
8.696687	555.151748	10.348391
8.786024	558.130186	10.353408
8.726181	561.462738	10.358426
8.929194	556.478833	10.363443
8.716357	546.166229	10.368461
8.417380	539.576852	10.373479
8.549465	548.917687	10.378496
8.646565	562.622280	10.383514
8.582386	550.993146	10.388531
8.478333	551.613773	10.393549
8.446815	553.815298	10.398567
8.910248	558.718124	10.403584
8.455257	558.212342	10.408602
8.447735	551.168972	10.413619
8.589645	554.236340	10.418637
8.609080	554.195845	10.423655
8.970345	550.901384	10.428672
8.585024	552.807708	10.433690
8.332213	547.880928	10.438707
8.664464	567.972322	10.443725
8.945061	585.149050	10.448743
8.936221	579.306134	10.453760
9.022328	573.940935	10.458778
9.183745	577.596302	10.463795
8.831857	559.466723	10.468813
8.831120	549.798751	10.473831
8.769989	552.531932	10.478848
8.993648	579.103550	10.483866
9.290632	563.319195	10.488883
9.081380	563.044204	10.493901
9.073849	558.567535	10.498919
8.877096	561.046414	10.503936
8.669880	565.343483	10.508954
8.910240	550.982383	10.513971
9.125028	539.960075	10.518989
8.817243	551.179531	10.524007
8.915500	547.660872	10.529024
8.580985	556.958668	10.534042
9.438776	575.192915	10.539059
9.043586	568.127693	10.544077
9.246518	557.365055	10.549095
9.216070	553.320925	10.554112
9.085862	556.249933	10.559130
8.968625	553.879748	10.564147
9.032560	550.849044	10.569165
8.982752	546.791583	10.574183
9.003428	545.189982	10.579200
8.815328	555.770302	10.584218
9.183587	559.264541	10.589235
9.090163	556.538621	10.594253
8.892060	563.615901	10.599271
9.207110	572.132287	10.604288
9.199512	584.502212	10.609306
9.138376	575.599072	10.614323
9.086859	569.187444	10.619341
8.726559	580.231582	10.624359
9.429008	585.987651	10.629376
9.024302	589.033568	10.634394
9.366411	587.971540	10.639411
9.325344	588.053914	10.644429
8.993289	585.328751	10.649447
9.427244	573.016616	10.654464
9.106392	587.765987	10.659482
8.859680	588.429774	10.664499
9.352877	585.717713	10.669517
9.450121	594.738514	10.674535
9.093626	580.080135	10.679552
9.025692	591.525383	10.684570
9.276364	590.087796	10.689587
9.300333	586.528266	10.694605
9.085924	592.791194	10.699623
9.100689	584.835844	10.704640
8.997862	594.603048	10.709658
8.841780	588.729354	10.714675
8.975737	590.927943	10.719693
9.012615	586.148415	10.724711
9.108470	582.920934	10.729728
9.010666	589.861891	10.734746
9.140737	607.199220	10.739763
9.577767	609.365538	10.744781
9.469331	618.381079	10.749799
9.662114	607.048248	10.754816
9.510909	591.710197	10.759834
9.107613	582.572809	10.764851
9.431323	589.131672	10.769869
9.221132	588.686300	10.774887
9.258861	602.236009	10.779904
9.436211	614.603932	10.784922
9.565949	609.798326	10.789939
9.589272	610.726187	10.794957
9.390518	609.697151	10.799975
9.262985	599.162583	10.804992
9.490496	625.641637	10.810010
9.302822	618.351979	10.815027
9.365790	614.552875	10.820045
9.306452	616.004039	10.825063
9.579807	606.992959	10.830080
9.541891	621.121902	10.835098
9.674619	618.803983	10.840115
9.744760	609.559705	10.845133
9.463601	623.976929	10.850151
9.424474	619.207392	10.855168
9.476796	618.780043	10.860186
9.415177	619.699210	10.865203
9.793064	617.060617	10.870221
9.709912	613.124472	10.875239
9.880291	623.297538	10.880256
9.748456	621.672914	10.885274
9.717257	606.325742	10.890291
9.530613	589.021898	10.895309
8.988843	598.784196	10.900327
9.627366	608.576210	10.905344
9.633615	622.933341	10.910362
9.799280	624.139982	10.915379
9.585785	614.025434	10.920397
9.467921	629.670741	10.925415
9.701892	620.683579	10.930432
9.670059	619.216016	10.935450
9.529499	614.065882	10.940467
10.006870	620.820385	10.945485
9.720037	617.517877	10.950503
9.755159	619.228376	10.955520
9.779544	615.197212	10.960538
9.561275	629.381847	10.965555
9.762861	618.428088	10.970573
9.780761	625.977375	10.975591
9.743315	629.823952	10.980608
9.813246	622.811934	10.985626
9.336490	627.209852	10.990643
9.620403	626.922542	10.995661
9.561452	620.769156	11.000679
9.733025	622.912331	11.005696
9.614665	626.230457	11.010714
9.662353	621.660901	11.015731
9.656863	621.587328	11.020749
9.625738	626.382670	11.025767
9.735834	627.095445	11.030784
9.812918	633.169795	11.035802
10.096403	639.274002	11.040819
10.298789	634.285943	11.045837
9.870136	630.709881	11.050855
9.652718	617.288763	11.055872
9.853509	612.962458	11.060890
9.741303	611.899143	11.065907
9.794508	618.429114	11.070925
9.780072	641.797922	11.075943
10.311935	642.386679	11.080960
10.360324	633.405182	11.085978
10.093116	629.235132	11.090995
10.063566	615.216450	11.096013
9.775088	624.294909	11.101031
9.718487	617.291896	11.106048
10.343778	622.097143	11.111066
9.900068	622.674121	11.116083
10.193918	615.626578	11.121101
9.985833	615.656057	11.126119
10.088368	612.833487	11.131136
10.437077	615.490488	11.136154
10.101079	618.257688	11.141171
10.343950	617.638153	11.146189
10.025356	622.425794	11.151207
10.041742	618.393884	11.156224
10.463533	616.220677	11.161242
9.891824	620.145307	11.166259
10.194063	617.612405	11.171277
10.075505	618.199220	11.176295
10.074038	614.421884	11.181312
10.388056	606.482903	11.186330
9.859798	612.673910	11.191347
9.818104	623.436537	11.196365
9.647113	621.649814	11.201383
9.881180	614.910911	11.206400
10.333746	632.774780	11.211418
10.238990	640.999057	11.216435
10.344424	642.077689	11.221453
10.049574	649.326870	11.226471
9.926254	647.879245	11.231488
10.160677	643.152864	11.236506
10.470632	645.196418	11.241523
10.555231	641.799656	11.246541
10.377194	645.742192	11.251559
10.081978	642.860961	11.256576
10.402601	643.413775	11.261594
9.883831	646.235490	11.266611
10.151239	644.961339	11.271629
10.301000	637.409258	11.276647
10.419428	649.422944	11.281664
10.785258	647.033140	11.286682
10.353395	646.085430	11.291699
10.696614	634.094775	11.296717
10.157790	636.676445	11.301735
10.188388	642.051534	11.306752
10.521446	638.757977	11.311770
10.287701	646.883595	11.316787
10.198880	639.256101	11.321805
10.061491	643.813548	11.326823
10.145168	644.684006	11.331840
10.131005	637.654979	11.336858
10.224360	649.220240	11.341875
10.258235	645.483996	11.346893
10.068219	645.727375	11.351911
9.977635	657.199836	11.356928
10.448287	667.279519	11.361946
10.163948	678.059353	11.366963
10.946655	668.921650	11.371981
10.818657	671.848937	11.376999
10.901018	674.394384	11.382016
10.606818	640.943227	11.387034
10.550370	647.264998	11.392051
10.411354	653.967666	11.397069
10.403212	649.139960	11.402087
10.170431	656.125886	11.407104
10.461794	659.704790	11.412122
10.689994	682.271410	11.417139
10.921245	679.801696	11.422157
10.957383	675.984869	11.427175
10.742350	662.457040	11.432192
10.604183	644.748743	11.437210
10.681567	650.208211	11.442227
10.634863	645.116066	11.447245
10.698366	631.256956	11.452263
10.405978	639.719757	11.457280
10.504546	641.472126	11.462298
10.839736	664.932276	11.467315
10.682569	665.005496	11.472333
10.816415	641.537729	11.477351
10.571667	656.445520	11.482368
10.803551	664.180188	11.487386
10.701518	665.406765	11.492403
11.057807	669.179724	11.497421
10.896917	645.547706	11.502439
10.801658	651.023994	11.507456
10.725612	636.321774	11.512474
10.632893	637.949781	11.517491
10.471542	650.583506	11.522509
11.057505	668.886404	11.527527
10.496430	675.356722	11.532544
10.881444	676.276775	11.537562
10.802727	688.428463	11.542579
11.186376	672.118751	11.547597
11.213887	662.234960	11.552615
10.718237	660.325541	11.557632
11.114954	638.251948	11.562650
10.695770	646.002878	11.567667
10.830778	658.573759	11.572685
11.031845	663.240012	11.577703
10.936846	662.101817	11.582720
11.030566	657.963041	11.587738
10.831103	651.147861	11.592755
10.741570	668.682935	11.597773
11.322866	671.410839	11.602791
10.723681	664.489203	11.607808
11.044851	673.945196	11.612826
10.935644	678.544345	11.617843
10.646416	670.257471	11.622861
11.023246	672.572697	11.627879
10.982568	677.966367	11.632896
11.066796	667.954325	11.637914
10.994771	676.823359	11.642931
11.024060	675.092492	11.647949
11.256461	660.991117	11.652967
11.098597	674.081478	11.657984
10.985127	674.136259	11.663002
11.341173	665.041119	11.668019
11.028966	675.938232	11.673037
11.046072	671.772259	11.678055
11.050701	669.922558	11.683072
11.285177	687.607318	11.688090
10.906122	670.441851	11.693107
10.814174	679.355411	11.698125
11.304730	670.923535	11.703143
10.631548	681.858458	11.708160
10.907039	672.167198	11.713178
11.169726	679.962716	11.718195
10.584740	666.041286	11.723213
11.304347	685.683957	11.728231
11.376406	702.083822	11.733248
11.265492	695.713250	11.738266
11.512378	699.220198	11.743283
11.572065	683.806660	11.748301
11.472635	666.894339	11.753319
11.109104	679.478247	11.758336
11.508862	677.040517	11.763354
11.278704	664.896902	11.768371
11.195774	677.370180	11.773389
11.308826	666.430131	11.778407
11.175049	672.849813	11.783424
10.985321	664.840535	11.788442
11.122003	678.861462	11.793459
11.329648	689.830126	11.798477
11.624536	697.003523	11.803495
11.539051	711.433857	11.808512
11.657197	691.976688	11.813530
11.601750	686.255389	11.818547
11.278411	678.132383	11.823565
11.647861	664.837820	11.828583
11.610932	671.569188	11.833600
11.388390	671.809677	11.838618
11.567184	662.855816	11.843635
11.407606	667.378066	11.848653
11.490771	670.142037	11.853671
11.341419	672.088794	11.858688
11.633420	667.209022	11.863706
11.433320	661.995891	11.868723
11.160249	664.792161	11.873741
11.456347	676.510615	11.878759
11.423709	687.267361	11.883776
11.418253	691.926618	11.888794
11.570255	686.883692	11.893811
11.580470	700.493536	11.898829
11.910631	686.600840	11.903847
11.586344	704.794215	11.908864
11.636701	700.646750	11.913882
11.639139	692.228708	11.918899
11.691756	707.145270	11.923917
11.776428	693.430216	11.928935
11.461074	701.599758	11.933952
11.921622	708.332970	11.938970
12.011324	696.407187	11.943987
11.711245	703.919412	11.949005
11.920534	702.987179	11.954023
11.831423	685.432016	11.959040
11.492125	678.043985	11.964058
11.899027	688.228687	11.969075
11.597312	689.128983	11.974093
11.897519	685.850194	11.979111
11.942351	695.816737	11.984128
11.448410	686.688066	11.989146
11.790113	687.524350	11.994163
11.930266	706.175812	11.999181
11.794010	695.776944	12.004199
11.563314	705.978851	12.009216
11.735095	697.762895	12.014234
11.958732	695.666706	12.019251
11.610838	707.521718	12.024269
11.919349	690.226959	12.029287
11.916694	701.487913	12.034304
11.600430	703.539014	12.039322
11.983486	690.681661	12.044339
11.811574	701.133840	12.049357
11.863605	701.786838	12.054375
11.711227	699.546626	12.059392
11.516946	700.508288	12.064410
11.704240	699.728774	12.069427
11.458526	705.094440	12.074445
12.223051	712.985454	12.079463
12.722098	720.722842	12.084480
12.194440	708.450438	12.089498
12.275611	690.471143	12.094515
11.648242	709.341258	12.099533
12.100230	697.785738	12.104551
12.021593	696.098782	12.109568
11.991110	699.282839	12.114586
11.668678	693.933053	12.119603
11.844107	707.301469	12.124621
11.936811	715.229701	12.129639
12.480012	726.401256	12.134656
12.261389	724.529890	12.139674
12.378358	707.016420	12.144691
12.126037	705.006166	12.149709
12.213538	685.729429	12.154727
12.371364	682.868384	12.159744
12.089962	698.763381	12.164762
12.358698	698.033782	12.169779
12.225987	692.630602	12.174797
12.479553	685.220466	12.179815
12.308286	689.269846	12.184832
12.183912	682.718468	12.189850
12.377529	688.468130	12.194867
12.055169	689.066878	12.199885
12.137597	693.106514	12.204903
11.979054	693.508539	12.209920
12.016858	693.866898	12.214938
12.146127	706.202495	12.219955
12.507370	716.828338	12.224973
12.735915	715.591208	12.229991
12.435596	708.313628	12.235008
11.932419	703.289517	12.240026
12.450211	706.386611	12.245043
12.459231	721.011730	12.250061
12.554401	719.620887	12.255079
12.279077	719.767658	12.260096
12.352190	726.119320	12.265114
12.622133	718.297584	12.270131
12.544944	733.237099	12.275149
12.588348	722.718284	12.280167
12.522321	718.033659	12.285184
12.391953	710.037870	12.290202
12.664121	719.579337	12.295219
12.377146	714.253010	12.300237
12.398699	711.322666	12.305255
12.365398	713.832913	12.310272
12.574257	725.037282	12.315290
12.654823	715.630422	12.320307
12.617049	724.916773	12.325325
12.453659	724.209381	12.330343
12.910367	715.554280	12.335360
12.507625	718.164843	12.340378
12.764002	725.316670	12.345395
12.615376	721.217433	12.350413
12.671260	719.542686	12.355431
12.720212	723.424507	12.360448
12.426500	718.576562	12.365466
12.651048	706.169718	12.370483
12.819030	720.776538	12.375501
12.600714	715.249334	12.380519
12.372496	707.183022	12.385536
12.198159	714.928065	12.390554
12.472303	718.125650	12.395571
12.693314	719.530594	12.400589
12.457320	719.257854	12.405607
12.813502	711.555998	12.410624
12.540584	725.122217	12.415642
12.385790	721.917922	12.420659
13.028170	729.394174	12.425677
12.723945	740.792082	12.430695
12.726754	734.523347	12.435712
12.874845	737.959639	12.440730
13.015004	729.649206	12.445747
12.571137	731.251999	12.450765
12.876562	730.117889	12.455783
13.035638	740.036355	12.460800
12.883253	742.112141	12.465818
12.993689	730.032640	12.470835
13.068091	739.534177	12.475853
13.116706	731.328322	12.480871
13.249933	711.351414	12.485888
13.124231	716.698825	12.490906
13.252997	715.284128	12.495923
13.128158	716.772203	12.500941
12.560746	715.289516	12.505959
13.044732	711.716327	12.510976
13.062722	714.025025	12.515994
13.148714	712.984451	12.521011
12.768014	709.629535	12.526029
12.837334	713.913126	12.531047
12.905978	708.852576	12.536064
12.948427	714.135887	12.541082
13.194172	722.564715	12.546099
13.113519	734.937288	12.551117
13.022894	741.684547	12.556135
13.357818	729.031634	12.561152
13.238925	738.257200	12.566170
13.066826	717.888502	12.571187
13.314078	730.094209	12.576205
13.302815	728.719576	12.581223
13.130169	717.792360	12.586240
13.185788	715.561367	12.591258
13.363165	723.908401	12.596275
13.229515	714.822812	12.601293
13.149953	724.743900	12.606311
13.316502	720.947826	12.611328
13.393118	735.867831	12.616346
13.201531	721.740028	12.621363
13.371954	725.949642	12.626381
13.368873	727.649246	12.631399
13.178812	714.717718	12.636416
13.126844	730.518053	12.641434
13.258494	723.777527	12.646451
13.460515	721.261465	12.651469
13.119116	739.540566	12.656487
13.463000	735.640788	12.661504
13.549699	744.852754	12.666522
13.437744	741.013444	12.671539
13.571131	737.542765	12.676557
13.268446	739.428764	12.681575
13.377970	729.528129	12.686592
13.284486	732.153915	12.691610
13.459135	736.181569	12.696627
13.326158	736.602299	12.701645
13.142845	729.396891	12.706663
13.247447	732.854145	12.711680
13.243441	734.997715	12.716698
13.100424	738.510258	12.721715
13.575435	734.979287	12.726733
13.778391	752.897240	12.731751
13.751628	741.673412	12.736768
13.956521	739.112000	12.741786
13.606139	733.201376	12.746803
13.774983	722.579269	12.751821
13.656145	730.125323	12.756839
13.879433	722.341997	12.761856
13.672038	730.730085	12.766874
13.970265	729.658964	12.771891
13.618601	743.394580	12.776909
13.581051	737.508031	12.781927
13.731763	719.908966	12.786944
13.688059	734.351803	12.791962
13.863560	730.072451	12.796979
13.652640	718.441164	12.801997
13.802109	733.027930	12.807015
13.927657	724.687047	12.812032
13.745159	737.777695	12.817050
13.501911	727.918531	12.822067
14.234171	732.714796	12.827085
13.612525	732.855523	12.832103
13.676883	724.879506	12.837120
13.586075	725.365596	12.842138
13.590528	727.450887	12.847155
13.909717	723.807507	12.852173
13.484957	737.605482	12.857191
13.585127	749.374182	12.862208
13.919958	753.132405	12.867226
14.045165	758.704753	12.872243
14.456482	764.283454	12.877261
14.127110	763.539427	12.882279
14.159605	749.452899	12.887296
14.092945	732.170987	12.892314
14.039884	732.083133	12.897331
14.085364	722.885767	12.902349
14.098667	726.714535	12.907367
14.338834	716.322922	12.912384
14.052003	719.865820	12.917402
14.147091	713.975173	12.922419
14.076929	722.093775	12.927437
13.725816	728.613359	12.932455
13.956216	715.158696	12.937472
14.171330	725.021739	12.942490
14.257946	740.421303	12.947507
13.876080	728.782143	12.952525
14.047056	747.944507	12.957543
14.360662	744.308637	12.962560
14.084704	746.687861	12.967578
14.069461	752.299654	12.972595
14.185941	739.835262	12.977613
14.146075	749.899188	12.982631
14.254615	743.563674	12.987648
14.145586	751.879427	12.992666
14.255044	751.170046	12.997683
14.454874	756.281624	13.002701
14.374987	756.327214	13.007719
14.422730	759.968936	13.012736
14.221841	752.757269	13.017754
14.271257	752.906960	13.022771
14.139271	754.218202	13.027789
13.678287	758.943310	13.032807
14.350328	753.065158	13.037824
14.148002	751.219732	13.042842
14.037946	755.348859	13.047859
14.105341	752.979622	13.052877
14.571355	768.350270	13.057895
14.338880	780.125646	13.062912
14.597073	793.143615	13.067930
14.730173	782.132369	13.072947
14.884969	755.475151	13.077965
14.504680	761.858652	13.082983
14.472792	746.916396	13.088000
14.313501	743.345488	13.093018
14.268472	760.115780	13.098035
14.442294	759.336129	13.103053
14.687187	770.972780	13.108071
14.776508	769.515098	13.113088
14.938789	763.734663	13.118106
14.597380	765.276934	13.123123
14.685767	746.095331	13.128141
14.518228	748.959298	13.133159
14.420461	751.694533	13.138176
14.823821	758.961429	13.143194
14.695967	773.309175	13.148211
15.132105	765.844917	13.153229
14.522275	756.051431	13.158247
14.549409	759.180712	13.163264
14.720276	754.425142	13.168282
14.889190	764.274295	13.173299
14.882339	772.641172	13.178317
14.703040	761.744152	13.183335
14.641205	769.048074	13.188352
14.736061	777.226919	13.193370
14.823512	776.527964	13.198387
15.042822	777.484755	13.203405
15.088144	779.372293	13.208423
14.750871	766.514548	13.213440
14.803601	771.691573	13.218458
14.917759	779.653491	13.223475
14.878488	767.124676	13.228493
14.701082	775.847138	13.233511
15.076443	773.861568	13.238528
15.316054	770.216960	13.243546
15.141674	779.618913	13.248563
15.105559	769.804021	13.253581
14.524270	755.683412	13.258599
14.803758	775.670827	13.263616
15.093716	775.809305	13.268634
15.198970	774.134069	13.273651
15.436469	776.720026	13.278669
15.053594	779.524916	13.283687
15.052520	781.372591	13.288704
15.064781	780.719126	13.293722
14.850706	777.693678	13.298739
14.937088	768.088618	13.303757
15.129147	774.927044	13.308775
14.833436	765.126910	13.313792
14.974020	772.283526	13.318810
15.145675	773.832235	13.323827
15.068481	775.540155	13.328845
15.192810	775.586342	13.333863
14.953650	768.781802	13.338880
15.383898	770.081320	13.343898
14.784448	780.765099	13.348915
15.329924	778.773952	13.353933
15.306953	779.348912	13.358951
15.055340	772.271284	13.363968
15.489009	783.381370	13.368986
15.384853	797.071409	13.374003
15.476965	781.496046	13.379021
15.254705	778.909367	13.384039
15.410440	795.807219	13.389056
15.586227	778.974467	13.394074
15.427515	775.641304	13.399091
15.270511	778.491235	13.404109
15.596636	785.874923	13.409127
15.695729	789.388701	13.414144
15.640499	784.770959	13.419162
15.217470	779.831098	13.424179
15.483106	768.813409	13.429197
15.662135	774.023393	13.434215
15.250636	772.348825	13.439232
15.748658	784.522188	13.444250
15.411308	782.943120	13.449267
15.602754	782.098460	13.454285
15.621830	799.351120	13.459303
15.768755	794.507878	13.464320
15.947688	775.620764	13.469338
15.555577	773.278452	13.474355
15.685545	770.362753	13.479373
15.289583	765.084138	13.484391
15.220068	774.454686	13.489408
15.881620	782.883620	13.494426
15.819464	793.863880	13.499443
15.733740	795.735288	13.504461
16.164318	794.623594	13.509479
15.910444	792.088388	13.514496
16.046457	771.561143	13.519514
15.672726	784.911933	13.524531
15.865031	768.092109	13.529549
15.890790	761.980760	13.534567
15.673159	767.213287	13.539584
15.651385	768.844049	13.544602
15.729808	770.023100	13.549619
15.878935	788.162351	13.554637
15.751785	789.958434	13.559655
15.879601	797.482360	13.564672
15.925394	792.914739	13.569690
16.162332	805.602828	13.574707
15.844179	801.731449	13.579725
16.110135	790.230713	13.584743
15.847565	799.593817	13.589760
16.039068	791.327907	13.594778
16.121005	793.721209	13.599795
16.024572	797.304202	13.604813
16.151335	795.577978	13.609831
15.749663	801.978314	13.614848
16.092243	800.859709	13.619866
16.159685	804.002610	13.624883
16.211059	796.084006	13.629901
16.339752	797.175633	13.634919
16.325344	801.361688	13.639936
16.387936	788.089289	13.644954
16.042296	789.977865	13.649971
15.850208	796.860692	13.654989
16.073565	793.123507	13.660007
15.951742	798.332635	13.665024
16.023013	794.556913	13.670042
16.130104	796.480201	13.675059
15.831985	801.648988	13.680077
16.314570	795.587405	13.685095
16.314798	800.725587	13.690112
16.444727	797.711285	13.695130
16.444603	796.204811	13.700147
16.249869	798.164594	13.705165
16.434670	805.794439	13.710183
16.196582	803.583333	13.715200
16.243260	796.719146	13.720218
16.320567	805.488886	13.725235
16.249658	793.048037	13.730253
16.514091	794.700489	13.735271
16.149980	805.755455	13.740288
16.399311	788.183214	13.745306
16.613631	802.126181	13.750323
16.668005	809.598580	13.755341
16.560388	791.209109	13.760359
16.245404	799.441916	13.765376
16.554529	804.833818	13.770394
17.099618	805.670351	13.775411
16.484804	793.848615	13.780429
16.673726	787.259491	13.785447
16.363228	793.480222	13.790464
16.330672	789.756003	13.795482
16.754611	813.380521	13.800499
16.726040	814.144856	13.805517
17.082995	815.493197	13.810535
16.503761	812.443652	13.815552
16.699631	792.297851	13.820570
16.557299	799.872030	13.825587
16.641265	803.337828	13.830605
17.157252	800.898979	13.835623
16.756677	796.702013	13.840640
17.001710	784.685840	13.845658
16.844273	776.866898	13.850675
16.531273	783.847343	13.855693
16.566892	782.891649	13.860711
16.491303	800.827544	13.865728
16.789639	806.138568	13.870746
16.761530	799.345389	13.875763
16.420841	814.306484	13.880781
16.981515	815.134832	13.885799
16.532971	817.588051	13.890816
16.724860	810.172893	13.895834
16.730802	808.566614	13.900851
16.679338	801.114032	13.905869
17.088495	820.500856	13.910887
17.135250	822.769095	13.915904
17.092691	809.160479	13.920922
17.427959	808.757023	13.925939
16.807361	816.065033	13.930957
17.277203	795.182056	13.935975
16.947771	806.801657	13.940992
16.829281	813.021565	13.946010
17.528473	807.970246	13.951027
17.106505	814.177128	13.956045
17.074564	810.477502	13.961063
16.918995	822.475689	13.966080
17.365549	825.712904	13.971098
17.612436	827.477097	13.976115
17.300353	823.017220	13.981133
17.353741	805.986693	13.986151
17.252955	809.623548	13.991168
17.307435	803.219694	13.996186
17.367152	806.105456	14.001203
17.179316	810.211631	14.006221
17.281364	804.464752	14.011239
17.422722	814.758369	14.016256
17.396727	817.043452	14.021274
17.408112	811.657059	14.026291
17.164855	811.693236	14.031309
17.396899	812.659734	14.036327
17.495142	829.105596	14.041344
17.686848	837.121252	14.046362
17.465081	817.675616	14.051379
17.283144	826.719760	14.056397
17.770761	821.013667	14.061415
17.660196	823.199656	14.066432
17.149667	814.617839	14.071450
17.682462	820.527307	14.076467
17.391286	833.674572	14.081485
18.014949	839.392587	14.086503
17.717653	826.403995	14.091520
17.536117	810.437783	14.096538
17.763597	805.560462	14.101555
17.182971	805.415624	14.106573
17.738394	819.784136	14.111591
17.663749	829.749451	14.116608
17.765148	832.642697	14.121626
18.073853	834.526867	14.126643
17.567662	838.351567	14.131661
17.868372	837.835536	14.136679
17.894723	829.551827	14.141696
17.718309	824.485387	14.146714
17.919677	822.488316	14.151731
17.435890	826.977493	14.156749
17.636453	820.936526	14.161767
17.414596	833.365086	14.166784
17.368974	827.907119	14.171802
17.706781	823.178655	14.176819
17.691432	830.067618	14.181837
17.876928	828.033314	14.186855
17.941862	828.120019	14.191872
17.858384	831.052674	14.196890
17.864684	818.696468	14.201907
17.547231	823.010744	14.206925
18.037933	841.979175	14.211943
18.319303	848.757707	14.216960
18.280490	842.710234	14.221978
18.451432	827.321368	14.226995
18.156423	830.484512	14.232013
18.520669	820.628421	14.237031
18.113089	831.667366	14.242048
18.307066	822.526488	14.247066
18.684698	814.241321	14.252083
18.128602	823.975622	14.257101
18.385513	816.294842	14.262119
18.460650	822.614031	14.267136
18.346294	825.279692	14.272154
18.846810	814.069740	14.277171
18.324568	818.924159	14.282189
18.191787	803.410638	14.287207
18.446846	805.874232	14.292224
18.183003	807.591941	14.297242
18.467624	814.228805	14.302259
18.337415	808.376730	14.307277
18.421053	824.304232	14.312295
18.295765	812.590724	14.317312
18.294942	825.860048	14.322330
18.589013	821.848424	14.327347
18.343532	811.535132	14.332365
18.362135	819.137045	14.337383
18.536175	819.627787	14.342400
18.465936	816.218786	14.347418
18.563072	817.754720	14.352435
18.386143	817.775213	14.357453
18.202710	812.019514	14.362471
18.669520	819.500519	14.367488
18.136524	827.889622	14.372506
18.548837	812.672162	14.377523
18.264261	813.265949	14.382541
18.285416	822.583657	14.387559
18.690652	812.190189	14.392576
18.357076	824.023636	14.397594
18.474213	809.930840	14.402611
18.494669	819.827785	14.407629
18.501350	848.364501	14.412647
18.856511	851.798091	14.417664
18.774617	850.734670	14.422682
18.840902	848.774188	14.427699
18.869045	853.884845	14.432717
18.692374	849.844135	14.437735
18.709978	847.954088	14.442752
18.325605	850.306861	14.447770
18.990217	851.883249	14.452787
18.869740	856.326469	14.457805
18.643484	851.016039	14.462823
18.798057	849.900158	14.467840
19.048697	845.502569	14.472858
19.032852	850.431159	14.477875
18.639639	848.312402	14.482893
18.704158	848.549344	14.487911
19.163944	855.349764	14.492928
18.899289	837.880511	14.497946
19.216092	847.756253	14.502963
19.054060	851.679861	14.507981
18.784822	848.172857	14.512999
19.183137	847.149842	14.518016
19.136518	856.439014	14.523034
19.118441	855.976549	14.528051
18.834517	856.538642	14.533069
19.279270	875.750098	14.538087
19.746267	864.291759	14.543104
19.439134	859.663860	14.548122
19.502274	852.898089	14.553139
19.310423	839.797294	14.558157
19.168156	839.295422	14.563175
19.547800	835.141823	14.568192
19.271539	838.127691	14.573210
19.682461	840.813224	14.578227
19.428702	851.971717	14.583245
19.499623	844.262515	14.588263
19.613469	844.566883	14.593280
19.349117	847.530611	14.598298
19.526663	842.552298	14.603315
19.470418	840.109304	14.608333
19.486167	839.913836	14.613351
19.841296	846.109516	14.618368
19.210181	854.346080	14.623386
19.852662	839.856656	14.628403
19.569906	839.283923	14.633421
19.190139	844.543073	14.638439
19.645299	838.098675	14.643456
19.293774	843.472427	14.648474
19.358736	840.804519	14.653491
19.467617	841.932587	14.658509
19.533687	843.168300	14.663527
19.597617	832.335741	14.668544
19.283876	843.142199	14.673562
19.756779	851.125466	14.678579
19.688609	867.548288	14.683597
19.760770	880.290240	14.688615
20.091829	869.046747	14.693632
19.873391	865.923496	14.698650
19.547339	844.981656	14.703667
19.678713	849.033122	14.708685
19.805254	870.774358	14.713703
20.213539	870.121083	14.718720
19.889288	877.232244	14.723738
20.194993	867.559388	14.728755
19.987386	839.253367	14.733773
19.857019	843.208348	14.738791
19.729525	830.529523	14.743808
19.992827	851.130131	14.748826
20.212789	857.488283	14.753843
19.876190	850.930179	14.758861
19.968531	859.892607	14.763879
20.028393	854.108202	14.768896
20.026236	860.945204	14.773914
20.038851	867.891068	14.778931
20.004495	866.893399	14.783949
20.154907	860.441883	14.788967
20.517055	864.458662	14.793984
20.418388	861.214457	14.799002
20.296130	864.207945	14.804019
20.692390	860.242503	14.809037
20.251550	846.702622	14.814055
20.259475	833.957821	14.819072
20.025064	842.915586	14.824090
20.162895	828.570383	14.829107
20.135739	833.250982	14.834125
20.111589	857.781155	14.839143
20.319057	851.011118	14.844160
20.357676	866.247019	14.849178
19.945863	862.638694	14.854195
20.089818	859.271439	14.859213
20.362350	867.323646	14.864231
20.384629	853.246977	14.869248
20.102152	858.151829	14.874266
20.034968	868.613188	14.879283
20.327453	849.783483	14.884301
20.246551	873.373825	14.889319
20.409911	891.166815	14.894336
20.717357	890.340572	14.899354
21.025022	876.264744	14.904371
21.129474	874.375792	14.909389
20.949222	858.212700	14.914407
20.907269	844.322606	14.919424
21.239429	860.441907	14.924442
21.156652	858.800195	14.929459
20.978894	843.485468	14.934477
20.890819	855.135582	14.939495
21.027681	844.651131	14.944512
21.087476	822.221019	14.949530
20.608029	821.876030	14.954547
20.714249	815.234727	14.959565
20.888658	820.593592	14.964583
20.868347	834.203187	14.969600
20.952632	836.550644	14.974618
20.528124	827.452729	14.979635
21.075297	834.242044	14.984653
21.175053	844.092443	14.989671
21.106928	840.188986	14.994688
20.986163	833.103581	14.999706
21.148976	819.348537	15.004723
20.831085	808.526542	15.009741
20.555220	830.049529	15.014759
20.650456	831.755432	15.019776
20.999796	840.825155	15.024794
20.984152	846.565174	15.029811
21.256734	841.783617	15.034829
20.915714	849.417322	15.039847
21.156695	849.291504	15.044864
21.171183	850.209228	15.049882
21.006251	850.868958	15.054899
21.397793	845.761106	15.059917
21.115153	853.780761	15.064935
21.178383	847.199787	15.069952
21.121109	836.265819	15.074970
20.814954	832.863228	15.079987
21.162754	848.891760	15.085005
21.048456	858.325361	15.090023
21.105774	865.167790	15.095040
21.498124	873.190852	15.100058
21.368194	873.929822	15.105075
21.607118	865.118635	15.110093
21.191761	871.340586	15.115111
21.607209	874.831725	15.120128
21.569007	875.035948	15.125146
21.252550	878.309320	15.130163
21.719307	862.596879	15.135181
21.420087	873.567266	15.140199
21.130954	870.530585	15.145216
21.362027	864.682160	15.150234
21.711750	873.174189	15.155251
21.828348	875.211447	15.160269
21.383823	877.617562	15.165287
21.652686	866.668450	15.170304
21.700654	870.131848	15.175322
21.257466	879.126791	15.180339
21.831729	864.013301	15.185357
21.649874	880.743159	15.190375
21.504009	874.044195	15.195392
21.589252	878.770493	15.200410
21.661939	895.183157	15.205427
22.298213	896.970298	15.210445
22.205206	897.749222	15.215463
22.031335	874.308036	15.220480
22.209079	864.250005	15.225498
22.154628	870.251714	15.230515
22.029194	865.772198	15.235533
21.649992	875.271038	15.240551
21.667713	858.053076	15.245568
21.735834	861.606234	15.250586
22.197271	893.032890	15.255603
22.250011	880.175054	15.260621
22.171486	879.907189	15.265639
22.093798	875.499392	15.270656
22.258721	863.173029	15.275674
21.957748	872.970694	15.280691
22.278716	868.727784	15.285709
21.929938	877.108613	15.290727
21.960631	889.520873	15.295744
22.188732	889.452291	15.300762
22.218357	903.323429	15.305779
22.536439	899.148103	15.310797
22.413741	902.645516	15.315815
22.374258	911.966903	15.320832
22.763494	899.830567	15.325850
22.271025	889.702204	15.330867
22.409712	883.951602	15.335885
22.314516	891.078156	15.340903
22.089281	903.354701	15.345920
22.375491	891.005321	15.350938
22.495002	903.305000	15.355955
22.606899	900.822992	15.360973
22.809852	897.867162	15.365991
22.300474	897.726785	15.371008
22.713723	898.173079	15.376026
22.592225	901.447598	15.381043
22.511140	906.493464	15.386061
22.449060	908.264146	15.391079
22.420548	898.888582	15.396096
22.455879	902.040549	15.401114
22.383550	906.102076	15.406131
22.612116	900.385327	15.411149
22.578141	903.275864	15.416167
22.447166	898.579085	15.421184
22.511520	897.154153	15.426202
22.401165	908.267930	15.431219
22.846844	910.938580	15.436237
22.735894	932.362914	15.441255
22.955388	920.456447	15.446272
23.358074	922.075635	15.451290
22.795637	930.709083	15.456307
22.902020	922.705353	15.461325
23.241246	912.016088	15.466343
22.601957	934.532672	15.471360
23.424106	918.032835	15.476378
22.786660	911.758926	15.481395
23.170991	922.685570	15.486413
23.052745	913.375998	15.491431
23.103190	918.510447	15.496448
23.155413	914.891163	15.501466
22.935580	914.194466	15.506483
23.182937	913.185470	15.511501
23.209556	917.575173	15.516519
23.069254	922.224506	15.521536
23.277476	909.850997	15.526554
23.056890	917.313286	15.531571
23.116228	920.458436	15.536589
23.121539	921.244929	15.541607
23.203306	924.698916	15.546624
23.145675	919.089385	15.551642
23.430150	925.322261	15.556659
22.974922	925.276853	15.561677
23.099990	925.966602	15.566695
23.121503	930.117431	15.571712
23.689439	932.895123	15.576730
23.413543	950.150741	15.581747
23.748094	935.699911	15.586765
23.462457	915.078894	15.591783
23.622176	925.793098	15.596800
23.415339	917.846051	15.601818
23.982276	939.684165	15.606835
23.312054	931.386892	15.611853
23.987178	929.347339	15.616871
23.603828	935.077007	15.621888
23.770073	922.344645	15.626906
23.610083	917.586033	15.631923
23.648868	921.885848	15.636941
23.893328	920.481241	15.641959
23.706687	928.668306	15.646976
23.774481	922.191251	15.651994
23.813280	931.574109	15.657011
23.705825	934.304187	15.662029
24.166569	936.164919	15.667047
23.673452	948.226660	15.672064
23.986299	943.372584	15.677082
23.977885	936.244750	15.682099
23.967153	940.443718	15.687117
24.318474	940.142214	15.692135
24.053457	945.539198	15.697152
24.181598	945.402210	15.702170
24.385806	945.333443	15.707187
24.069801	921.277795	15.712205
23.831204	915.674553	15.717223
24.089917	911.495945	15.722240
23.859265	922.086205	15.727258
24.151676	942.456379	15.732275
24.030065	939.201090	15.737293
24.146883	932.134439	15.742311
23.875162	942.267606	15.747328
23.925171	934.505231	15.752346
24.142493	938.171030	15.757363
24.128415	937.233281	15.762381
24.162973	939.323369	15.767399
24.048306	946.283020	15.772416
24.465503	946.815262	15.777434
24.481145	951.886982	15.782451
24.298157	952.463396	15.787469
24.913734	937.932665	15.792487
24.740405	943.493501	15.797504
24.845310	937.093559	15.802522
24.829282	933.844343	15.807539
24.739365	939.829995	15.812557
24.825661	923.662051	15.817575
24.662266	926.452938	15.822592
24.692321	937.121660	15.827610
24.657431	932.465380	15.832627
24.307888	930.672503	15.837645
24.232475	932.067800	15.842663
24.584443	928.872516	15.847680
24.568314	922.587151	15.852698
24.483682	934.759694	15.857715
24.860357	944.692916	15.862733
24.753316	949.348077	15.867751
24.885337	966.142576	15.872768
24.875027	957.100818	15.877786
24.982808	958.146709	15.882803
24.965747	962.365229	15.887821
25.004022	955.953362	15.892839
25.248724	953.227293	15.897856
24.794545	933.402076	15.902874
25.259942	936.033259	15.907891
24.616863	931.744463	15.912909
24.745799	944.120064	15.917927
25.306683	956.792044	15.922944
25.302812	947.725610	15.927962
25.355131	951.138217	15.932979
25.433784	959.790128	15.937997
25.268254	936.467427	15.943015
25.144469	929.008233	15.948032
25.121798	925.457513	15.953050
24.899672	935.568506	15.958067
25.409700	960.059773	15.963085
25.460521	948.515448	15.968103
25.374261	952.786831	15.973120
25.454718	960.938041	15.978138
25.622687	955.964719	15.983155
25.320059	950.396450	15.988173
25.766396	948.093575	15.993191
25.090631	941.965330	15.998208
25.370202	936.333134	16.003226
25.363250	945.014043	16.008243
25.329550	951.793711	16.013261
25.781021	949.208837	16.018279
25.287192	964.254330	16.023296
25.492633	960.246000	16.028314
25.760314	953.489585	16.033331
25.635194	951.562590	16.038349
25.743968	951.900076	16.043367
25.657953	946.708341	16.048384
25.627669	951.024696	16.053402
25.651578	951.863914	16.058419
25.592994	951.526229	16.063437
25.660910	940.079658	16.068455
25.531633	950.831205	16.073472
25.581781	962.158119	16.078490
25.793805	958.862355	16.083507
25.942254	972.300607	16.088525
26.158061	980.020872	16.093543
26.088743	974.412563	16.098560
26.019173	965.517971	16.103578
25.713875	960.325270	16.108595
25.822139	970.369388	16.113613
25.936505	980.897950	16.118631
26.101274	980.773212	16.123648
26.230924	982.180584	16.128666
26.301567	982.233773	16.133683
26.199297	989.548615	16.138701
26.540837	976.159398	16.143719
26.572260	982.682004	16.148736
26.024328	966.930873	16.153754
26.502337	971.033929	16.158771
25.898669	971.143146	16.163789
25.912361	967.685208	16.168807
26.051167	982.015653	16.173824
26.266357	978.230471	16.178842
26.222106	971.648114	16.183859
26.017202	985.490378	16.188877
26.437328	981.113455	16.193895
26.137710	978.480186	16.198912
26.168231	975.043378	16.203930
26.584827	976.175910	16.208947
26.342438	986.521249	16.213965
26.560923	986.197018	16.218983
26.554576	991.886647	16.224000
26.802814	1002.469368	16.229018
26.810665	995.739536	16.234035
27.056397	993.053145	16.239053
27.019672	978.734483	16.244071
27.007533	967.520176	16.249088
26.793899	968.749868	16.254106
26.809765	969.016305	16.259123
26.692579	960.329549	16.264141
27.247107	960.788910	16.269159
27.228684	962.126769	16.274176
26.959388	965.067128	16.279194
27.225509	951.108314	16.284211
26.889341	961.901438	16.289229
26.826309	961.921708	16.294247
26.694883	960.933382	16.299264
26.829646	970.385627	16.304282
26.935967	962.797462	16.309299
26.856616	971.592792	16.314317
26.679265	954.534985	16.319335
26.754247	966.357415	16.324352
26.896854	987.531302	16.329370
27.226716	998.537463	16.334387
27.173731	992.585858	16.339405
27.461339	988.978043	16.344423
27.279726	994.008666	16.349440
27.274010	995.710900	16.354458
27.469755	986.936891	16.359475
27.342846	997.129418	16.364493
27.248963	996.997825	16.369511
27.303407	985.707651	16.374528
27.291014	988.117261	16.379546
27.359213	988.843964	16.384563
27.203344	990.596990	16.389581
27.247958	985.745403	16.394599
27.251584	988.447885	16.399616
27.149522	990.341107	16.404634
27.651350	988.665853	16.409651
27.627757	1013.468183	16.414669
27.878573	1014.564050	16.419687
27.678546	1004.267324	16.424704
27.678013	1011.197023	16.429722
27.692421	995.648158	16.434739
27.760576	1013.987739	16.439757
27.974622	1022.148101	16.444775
27.905563	1010.244866	16.449792
27.796102	1012.820198	16.454810
27.857512	1005.013096	16.459827
27.718552	1002.838031	16.464845
27.565298	1013.228982	16.469863
28.026966	1018.171712	16.474880
27.724694	1018.119331	16.479898
27.822362	1015.347777	16.484915
27.712283	1023.487602	16.489933
27.950454	1021.730837	16.494951
28.158268	1014.769760	16.499968
28.574963	1014.164097	16.504986
28.641076	1015.339493	16.510003
28.442919	1017.042630	16.515021
28.313086	1011.725165	16.520039
28.328454	1017.531568	16.525056
28.387702	1012.041936	16.530074
28.585527	1008.890806	16.535091
28.216971	997.931404	16.540109
28.355829	985.548829	16.545127
28.168638	988.182073	16.550144
27.921361	1003.059128	16.555162
28.273426	999.886545	16.560179
28.384667	1023.765882	16.565197
28.522123	1035.678910	16.570215
28.420776	1014.636624	16.575232
28.335196	1013.090224	16.580250
28.378610	1013.566738	16.585267
28.381405	1017.687422	16.590285
28.385168	1016.513395	16.595303
28.492525	1020.596430	16.600320
28.423764	1015.100495	16.605338
28.712903	1002.317251	16.610355
28.602551	1011.665663	16.615373
28.504276	1012.924219	16.620391
28.838420	1016.809962	16.625408
28.832815	1033.497772	16.630426
28.819388	1015.302667	16.635443
28.594820	1014.752195	16.640461
28.458588	1025.669974	16.645479
28.657786	1019.799892	16.650496
28.701725	1022.513333	16.655514
29.327721	1022.364434	16.660531
29.465290	1022.305007	16.665549
29.052653	1026.451537	16.670567
29.410472	1018.712354	16.675584
29.115482	1026.285203	16.680602
29.112596	1023.540499	16.685619
29.245831	1022.709087	16.690637
29.174351	1016.865630	16.695655
29.553776	1015.629524	16.700672
29.058376	1026.182321	16.705690
29.070926	1002.602768	16.710707
29.478920	1006.888240	16.715725
29.070679	1029.735320	16.720743
29.198432	1019.185633	16.725760
28.992324	1024.320887	16.730778
28.959185	1017.169646	16.735795
29.041755	1021.325565	16.740813
29.290969	1021.822589	16.745831
29.078351	1011.618277	16.750848
29.171060	1049.221265	16.755866
29.533706	1048.842605	16.760883
29.729218	1056.696063	16.765901
29.663505	1056.150632	16.770919
29.815861	1056.017711	16.775936
29.566408	1047.709296	16.780954
29.558879	1053.913917	16.785971
29.835724	1057.208455	16.790989
29.988804	1051.990458	16.796007
29.918777	1046.019902	16.801024
30.141085	1052.670710	16.806042
29.939674	1048.295216	16.811059
30.393759	1047.031910	16.816077
29.681012	1033.583933	16.821095
30.055411	1013.165862	16.826112
29.393897	1023.064041	16.831130
29.593516	1033.306944	16.836147
30.221478	1035.927813	16.841165
30.268117	1053.530770	16.846183
30.460647	1048.197810	16.851200
30.143286	1046.435126	16.856218
30.269330	1045.495767	16.861235
30.113708	1036.342566	16.866253
30.126707	1045.579390	16.871271
30.576398	1028.482240	16.876288
30.060194	1037.215077	16.881306
29.953839	1033.009083	16.886323
30.223784	1036.072907	16.891341
30.245015	1038.419597	16.896359
30.356848	1033.808024	16.901376
30.075728	1043.970759	16.906394
30.269038	1037.933071	16.911411
30.339865	1046.324066	16.916429
30.304211	1042.504349	16.921447
30.184405	1036.189228	16.926464
29.967904	1044.787223	16.931482
30.241868	1043.674726	16.936499
30.485464	1057.152242	16.941517
30.385344	1069.657906	16.946535
30.357419	1063.060412	16.951552
30.752400	1061.228231	16.956570
30.971328	1062.316184	16.961587
31.120101	1057.723004	16.966605
31.128175	1063.734335	16.971623
31.000460	1066.051812	16.976640
31.204832	1059.047885	16.981658
31.120549	1039.901435	16.986675
31.042951	1034.234739	16.991693
31.304307	1031.172005	16.996711
31.391517	1025.747322	17.001728
31.087896	1030.759839	17.006746
30.806552	1023.235706	17.011763
30.953885	1032.310092	17.016781
30.641846	1028.385683	17.021799
30.874617	1033.860352	17.026816
30.969226	1038.597650	17.031834
31.076882	1050.046600	17.036851
31.239781	1059.143228	17.041869
30.704643	1070.241702	17.046887
30.756415	1062.841803	17.051904
31.076456	1067.843085	17.056922
31.341141	1057.504759	17.061939
31.270370	1050.107304	17.066957
31.205051	1060.768648	17.071975
30.941064	1053.582519	17.076992
30.781010	1069.168623	17.082010
31.149238	1079.001083	17.087027
31.769079	1087.874015	17.092045
31.863380	1092.760273	17.097063
32.153847	1089.617631	17.102080
31.913735	1088.684357	17.107098
31.363807	1088.054207	17.112115
31.839922	1092.177488	17.117133
31.529551	1091.465041	17.122151
31.869927	1086.555788	17.127168
31.947402	1093.807616	17.132186
32.009708	1092.778312	17.137203
31.932419	1083.611449	17.142221
31.870242	1086.959261	17.147239
32.161524	1083.061103	17.152256
31.978640	1064.645755	17.157274
31.731400	1056.011632	17.162291
31.920650	1062.509076	17.167309
31.670159	1072.676807	17.172327
32.131139	1077.082852	17.177344
32.213080	1074.219317	17.182362
31.941882	1087.048097	17.187379
31.982096	1073.712920	17.192397
31.900155	1087.067221	17.197415
32.159099	1081.759882	17.202432
32.506395	1076.097845	17.207450
32.136254	1080.605808	17.212467
32.219249	1070.881060	17.217485
32.308534	1079.698970	17.222503
32.402278	1082.719295	17.227520
32.557342	1074.976981	17.232538
32.306139	1087.498376	17.237555
32.327634	1084.659589	17.242573
32.322337	1074.243840	17.247591
32.235874	1079.775018	17.252608
32.383854	1069.685852	17.257626
32.298035	1082.536151	17.262643
32.765915	1088.772048	17.267661
32.661628	1088.450474	17.272679
32.516358	1099.180264	17.277696
33.178865	1097.967538	17.282714
32.739933	1084.995537	17.287731
32.866346	1083.817670	17.292749
32.300587	1072.714947	17.297767
32.440693	1082.532556	17.302784
32.957107	1094.669081	17.307802
32.758953	1097.795706	17.312819
32.998948	1105.569016	17.317837
32.545865	1103.830721	17.322855
32.840793	1102.224090	17.327872
32.863330	1108.016549	17.332890
32.765977	1110.267412	17.337907
32.866707	1096.481344	17.342925
33.024258	1101.720871	17.347943
33.233055	1118.960351	17.352960
33.156054	1110.472642	17.357978
33.161983	1124.520210	17.362995
33.495249	1126.240150	17.368013
33.654575	1116.507679	17.373031
33.298562	1093.864336	17.378048
33.705560	1092.815860	17.383066
33.658159	1086.855128	17.388083
33.548544	1077.217313	17.393101
33.591261	1088.483651	17.398119
33.802101	1083.966215	17.403136
33.639930	1077.711514	17.408154
33.872530	1090.470231	17.413171
33.774299	1079.853927	17.418189
33.798665	1080.800835	17.423207
33.825861	1081.767547	17.428224
33.798522	1078.587086	17.433242
33.800126	1086.267520	17.438259
33.922028	1069.434791	17.443277
33.888576	1083.492176	17.448295
33.579198	1072.815706	17.453312
33.816315	1076.976313	17.458330
33.645640	1087.435733	17.463347
33.765518	1080.846872	17.468365
33.513744	1081.470970	17.473383
33.569596	1094.049879	17.478400
33.678621	1092.579266	17.483418
33.426512	1113.330152	17.488435
33.755041	1124.302870	17.493453
33.689173	1113.941191	17.498471
33.937373	1130.179654	17.503488
34.271386	1113.224440	17.508506
34.030357	1115.909804	17.513523
34.574170	1115.891888	17.518541
34.359204	1111.787861	17.523559
34.058984	1114.032295	17.528576
34.366780	1128.983564	17.533594
34.499178	1146.813361	17.538611
34.572520	1134.328617	17.543629
34.328952	1135.117082	17.548647
34.336834	1139.027445	17.553664
34.492590	1139.173246	17.558682
34.633027	1145.301690	17.563699
34.576311	1133.196057	17.568717
35.013142	1132.890162	17.573735
34.848035	1130.443952	17.578752
34.942590	1116.764577	17.583770
34.629442	1120.570532	17.588787
34.676435	1112.915929	17.593805
34.660467	1113.404031	17.598823
34.936103	1118.542568	17.603840
35.180699	1129.557501	17.608858
34.885014	1125.088723	17.613875
34.649466	1114.204584	17.618893
34.568188	1129.105207	17.623911
34.809995	1127.914960	17.628928
35.016035	1118.229878	17.633946
35.103407	1131.704640	17.638963
34.997265	1127.490318	17.643981
35.196974	1129.472446	17.648999
34.702364	1141.993760	17.654016
34.975692	1133.401894	17.659034
34.907683	1137.289174	17.664051
34.996288	1142.354510	17.669069
35.360936	1132.741421	17.674087
35.442020	1149.201976	17.679104
35.683723	1158.061859	17.684122
35.682979	1144.735553	17.689139
35.570842	1130.303444	17.694157
35.617486	1121.103876	17.699175
35.375549	1133.456285	17.704192
35.443349	1120.595759	17.709210
35.187830	1126.890398	17.714227
35.665100	1145.551244	17.719245
36.049327	1143.759604	17.724263
35.897619	1150.043002	17.729280
36.126136	1139.482880	17.734298
35.733515	1125.560040	17.739315
36.008920	1122.598592	17.744333
36.163641	1113.147743	17.749351
36.009492	1117.386401	17.754368
36.153013	1103.370851	17.759386
35.829325	1123.303404	17.764403
35.510708	1120.718615	17.769421
35.924169	1121.529192	17.774439
35.931710	1146.852194	17.779456
36.079904	1152.874062	17.784474
35.791632	1147.540021	17.789491
35.905239	1153.804180	17.794509
36.284484	1161.796593	17.799527
36.023561	1153.305007	17.804544
36.355011	1146.938986	17.809562
36.280780	1159.135771	17.814579
36.393290	1148.241525	17.819597
36.140358	1146.147566	17.824615
36.202728	1151.084977	17.829632
36.618128	1145.930867	17.834650
36.558621	1150.016122	17.839667
36.389482	1146.977367	17.844685
36.390961	1151.497944	17.849703
36.195257	1161.592910	17.854720
36.830246	1158.229177	17.859738
36.910012	1166.160273	17.864755
37.123609	1168.637864	17.869773
36.969643	1141.651728	17.874791
36.816987	1147.296805	17.879808
36.892679	1139.547500	17.884826
36.918730	1129.646919	17.889843
37.138354	1136.709950	17.894861
37.320544	1137.963206	17.899879
36.975556	1137.045488	17.904896
37.038419	1142.513240	17.909914
37.058272	1145.514100	17.914931
36.714903	1146.770558	17.919949
37.070881	1147.746515	17.924967
37.499304	1139.292965	17.929984
37.366368	1134.838425	17.935002
37.094760	1148.436488	17.940019
37.247627	1139.562803	17.945037
37.194334	1123.865475	17.950055
37.145900	1134.301971	17.955072
37.257486	1128.476538	17.960090
37.012658	1124.469553	17.965107
36.792366	1139.437048	17.970125
37.440740	1142.116168	17.975143
37.353681	1154.926779	17.980160
37.152474	1164.903976	17.985178
37.513981	1162.768311	17.990195
37.184655	1148.488591	17.995213
37.778490	1158.036224	18.000231
37.547442	1159.788407	18.005248
37.443589	1145.882583	18.010266
37.457184	1162.352928	18.015283
37.615892	1188.655382	18.020301
37.832045	1184.709190	18.025319
37.447533	1199.808391	18.030336
37.668416	1177.050894	18.035354
37.700393	1189.277979	18.040371
37.674477	1189.683095	18.045389
37.834187	1183.841816	18.050407
38.010058	1187.651215	18.055424
38.106493	1188.511429	18.060442
38.310259	1182.597526	18.065459
38.362147	1189.858548	18.070477
38.346746	1180.394439	18.075495
38.028101	1189.488450	18.080512
38.613784	1181.561753	18.085530
38.414388	1179.860058	18.090547
38.324734	1192.136177	18.095565
38.190728	1183.079791	18.100583
38.348543	1196.699637	18.105600
38.053443	1217.656752	18.110618
38.552210	1205.353773	18.115635
38.164005	1206.585169	18.120653
38.705069	1212.347288	18.125671
38.349400	1209.105918	18.130688
38.601901	1209.586463	18.135706
38.763327	1201.784973	18.140723
38.968465	1211.339204	18.145741
38.924853	1204.739714	18.150759
38.596632	1211.273333	18.155776
38.833969	1211.441868	18.160794
39.039590	1203.674603	18.165811
39.132034	1205.319996	18.170829
39.367717	1196.191096	18.175847
39.147304	1210.219659	18.180864
39.212637	1202.375987	18.185882
39.326131	1208.017649	18.190899
39.125965	1206.045256	18.195917
39.454404	1197.071866	18.200935
39.159966	1208.248951	18.205952
39.168907	1204.812116	18.210970
39.335567	1201.044740	18.215987
39.051785	1207.720202	18.221005
38.971789	1203.926667	18.226023
39.088307	1204.188580	18.231040
39.112249	1200.994700	18.236058
39.537410	1207.540019	18.241075
39.147792	1227.659165	18.246093
39.511080	1233.358361	18.251111
39.465269	1244.606180	18.256128
39.732019	1239.134334	18.261146
40.065504	1235.117567	18.266163
39.774565	1235.887885	18.271181
39.929774	1226.659685	18.276199
39.966094	1218.907202	18.281216
39.917106	1215.985761	18.286234
39.831342	1206.414582	18.291251
39.488764	1216.673990	18.296269
40.189003	1221.979367	18.301287
40.013926	1213.895933	18.306304
39.794024	1223.321426	18.311322
40.010669	1222.780305	18.316339
40.103775	1232.355031	18.321357
40.061214	1218.260301	18.326375
40.055807	1226.672948	18.331392
39.844879	1217.557021	18.336410
40.187630	1221.994456	18.341427
40.105571	1228.662376	18.346445
40.357005	1220.237045	18.351463
40.110049	1230.613317	18.356480
39.961335	1238.096851	18.361498
40.482343	1238.364156	18.366515
40.410477	1254.952840	18.371533
40.498480	1255.031701	18.376551
40.840129	1247.103178	18.381568
40.533492	1251.396791	18.386586
40.855212	1250.213603	18.391603
40.551228	1247.137081	18.396621
41.067249	1260.864692	18.401639
40.923211	1249.937190	18.406656
40.730245	1238.648548	18.411674
40.952321	1246.152493	18.416691
40.639477	1246.768975	18.421709
40.821189	1239.818112	18.426727
40.568624	1245.452770	18.431744
40.325891	1247.356279	18.436762
40.847902	1246.105156	18.441779
40.608564	1255.147917	18.446797
41.140267	1265.853145	18.451815
41.208264	1271.680470	18.456832
41.263899	1285.867587	18.461850
41.547002	1281.305283	18.466867
41.383358	1276.633764	18.471885
41.363431	1282.480149	18.476903
41.468558	1264.432257	18.481920
41.568379	1279.467049	18.486938
41.705842	1271.765729	18.491955
41.690686	1263.205914	18.496973
41.393262	1262.789302	18.501991
41.846621	1263.309875	18.507008
41.703801	1271.912157	18.512026
41.724046	1263.311654	18.517043
41.848245	1261.988691	18.522061
41.667537	1263.870340	18.527079
41.527238	1264.823607	18.532096
41.792396	1262.404882	18.537114
41.908328	1253.827739	18.542131
41.798997	1275.496047	18.547149
41.613291	1261.181860	18.552167
42.177032	1255.413136	18.557184
41.865083	1270.143385	18.562202
41.862767	1255.208834	18.567219
41.847271	1260.883247	18.572237
41.968002	1268.962131	18.577255
42.266829	1279.658614	18.582272
42.106503	1291.972865	18.587290
42.284253	1293.420341	18.592307
42.285182	1294.465411	18.597325
42.647289	1288.566044	18.602343
42.734960	1288.831151	18.607360
42.207501	1294.939533	18.612378
42.883028	1281.554299	18.617395
42.408235	1292.570530	18.622413
42.410349	1294.532782	18.627431
42.713108	1290.659442	18.632448
42.791057	1285.396902	18.637466
43.114642	1287.934277	18.642483
42.789505	1289.624869	18.647501
42.821994	1289.112407	18.652519
42.679144	1276.064154	18.657536
42.499884	1286.915225	18.662554
42.805208	1284.898260	18.667571
42.968015	1288.888556	18.672589
42.734564	1283.901849	18.677607
42.950678	1284.011303	18.682624
42.894988	1290.764445	18.687642
42.714327	1289.062988	18.692659
42.867144	1285.058940	18.697677
42.789645	1311.138079	18.702695
43.047569	1302.933054	18.707712
43.152280	1319.814232	18.712730
43.146546	1309.899106	18.717747
43.341894	1310.207631	18.722765
43.196176	1319.529205	18.727783
43.357719	1306.610125	18.732800
43.350878	1314.484361	18.737818
43.081989	1318.685351	18.742835
43.597420	1330.128042	18.747853
43.468271	1321.044399	18.752871
43.755158	1325.748339	18.757888
43.861504	1326.911404	18.762906
44.009467	1317.979774	18.767923
44.230181	1329.946881	18.772941
43.846715	1327.806957	18.777959
44.327989	1313.159704	18.782976
43.821312	1331.003997	18.787994
44.209094	1324.971259	18.793011
44.288685	1321.208795	18.798029
44.251997	1325.971324	18.803047
44.546750	1317.801340	18.808064
44.195712	1307.843881	18.813082
44.162073	1299.849217	18.818099
43.971216	1307.213785	18.823117
44.315968	1309.109182	18.828135
44.354704	1321.465944	18.833152
44.438441	1326.099338	18.838170
44.277409	1324.165534	18.843187
44.573702	1326.105353	18.848205
44.300307	1322.932830	18.853223
44.425878	1316.982199	18.858240
44.382904	1327.918241	18.863258
44.596501	1323.868909	18.868275
44.669101	1311.237906	18.873293
44.224395	1324.516357	18.878311
44.539010	1322.623620	18.883328
44.522168	1342.140846	18.888346
44.538465	1344.947284	18.893363
44.914195	1345.213209	18.898381
44.848892	1363.818925	18.903399
45.074793	1351.976016	18.908416
44.742246	1352.124373	18.913434
44.849734	1351.877426	18.918451
45.052418	1344.264686	18.923469
44.943176	1343.143653	18.928487
45.049273	1346.119870	18.933504
45.181422	1363.064661	18.938522
45.203791	1360.659274	18.943539
45.754408	1359.638813	18.948557
45.576480	1368.308555	18.953575
45.710917	1343.501038	18.958592
45.546567	1339.892446	18.963610
45.548218	1334.899937	18.968627
45.858404	1332.543632	18.973645
45.594853	1337.263940	18.978663
45.789850	1336.034571	18.983680
45.754199	1333.003637	18.988698
45.600504	1341.964984	18.993715
45.927943	1335.323213	18.998733
45.904074	1358.786097	19.003751
46.097134	1352.994943	19.008768
45.941541	1348.561207	19.013786
45.603282	1349.067344	19.018803
46.136745	1354.577859	19.023821
45.739214	1366.882950	19.028839
46.330430	1373.263520	19.033856
46.450573	1375.061614	19.038874
45.923433	1375.245867	19.043891
46.234632	1373.109237	19.048909
46.316336	1370.135269	19.053927
46.354894	1365.375198	19.058944
46.243148	1367.249007	19.063962
45.936326	1365.427465	19.068979
46.568788	1368.658976	19.073997
45.990128	1366.024807	19.079015
46.460578	1368.265134	19.084032
46.649312	1396.148176	19.089050
46.683873	1393.296150	19.094067
46.911862	1385.630987	19.099085
47.009170	1387.570040	19.104103
47.202753	1390.559166	19.109120
46.832822	1388.799814	19.114138
46.985798	1393.014564	19.119155
46.854858	1385.045775	19.124173
47.027142	1389.676758	19.129191
46.928540	1379.132541	19.134208
47.183670	1380.755007	19.139226
46.939191	1380.026341	19.144243
47.068410	1378.759617	19.149261
47.070223	1380.061201	19.154279
47.290345	1380.169010	19.159296
47.215037	1377.561881	19.164314
46.832948	1382.896781	19.169331
47.141955	1379.777982	19.174349
47.372865	1407.567671	19.179367
47.655338	1399.188288	19.184384
47.736334	1402.234598	19.189402
47.647019	1407.128665	19.194419
48.056674	1408.168987	19.199437
47.903412	1401.476722	19.204455
47.812189	1402.084142	19.209472
48.432819	1406.184811	19.214490
48.089026	1393.371799	19.219507
48.209721	1369.927724	19.224525
47.526122	1384.945645	19.229543
47.675912	1380.587795	19.234560
48.083665	1390.731791	19.239578
47.948698	1403.379488	19.244595
48.102869	1391.905829	19.249613
47.638094	1402.876002	19.254631
47.760549	1394.632102	19.259648
47.931605	1390.597065	19.264666
48.099698	1403.334228	19.269683
48.460479	1390.688801	19.274701
48.118088	1397.448232	19.279719
48.298496	1413.062664	19.284736
48.752460	1430.242300	19.289754
48.915510	1426.692954	19.294771
48.600417	1417.455755	19.299789
48.779540	1425.606556	19.304807
48.750063	1427.894666	19.309824
48.976373	1431.871357	19.314842
48.724055	1420.521926	19.319859
48.340128	1408.059381	19.324877
48.115466	1423.883260	19.329895
48.653144	1419.827389	19.334912
48.461806	1417.224468	19.339930
48.565505	1432.932883	19.344947
49.164596	1434.256228	19.349965
49.206134	1455.610137	19.354983
49.477348	1452.331255	19.360000
49.528890	1446.403829	19.365018
49.707740	1458.160859	19.370035
49.750963	1439.313266	19.375053
49.467567	1431.819187	19.380071
49.100210	1429.342777	19.385088
49.167370	1430.061210	19.390106
49.384089	1451.920143	19.395123
49.563041	1452.036330	19.400141
49.573987	1450.188444	19.405159
49.634465	1451.619493	19.410176
49.609807	1449.956993	19.415194
49.664010	1443.507354	19.420211
49.895477	1439.990196	19.425229
49.772591	1454.432133	19.430247
49.738891	1444.773670	19.435264
50.070488	1444.284993	19.440282
49.393945	1456.737231	19.445299
49.836294	1463.283167	19.450317
49.895564	1475.638234	19.455335
50.266989	1484.039138	19.460352
50.382681	1479.663867	19.465370
50.335928	1486.112905	19.470387
50.492592	1487.297781	19.475405
50.868658	1478.140006	19.480423
50.554313	1483.237794	19.485440
50.553534	1470.599498	19.490458
50.485412	1483.104147	19.495475
50.753512	1475.930271	19.500493
50.614354	1478.016270	19.505511
50.389781	1468.654845	19.510528
50.667502	1477.213532	19.515546
50.638048	1473.724525	19.520563
50.639284	1471.115556	19.525581
50.817397	1466.283581	19.530599
50.917150	1462.765549	19.535616
50.918054	1472.305078	19.540634
50.698913	1466.038965	19.545651
51.060557	1471.875314	19.550669
51.405031	1492.081931	19.555687
51.525711	1503.917498	19.560704
51.649678	1487.642946	19.565722
51.161009	1472.267761	19.570739
51.141543	1468.002610	19.575757
51.266844	1460.872021	19.580775
51.214836	1485.653337	19.585792
51.392761	1475.522544	19.590810
51.445357	1500.063993	19.595827
51.522782	1495.920599	19.600845
51.832932	1488.688201	19.605863
51.544907	1492.350351	19.610880
51.584093	1488.075896	19.615898
51.236325	1485.584825	19.620915
51.271057	1491.408087	19.625933
51.552356	1506.991771	19.630951
51.911882	1510.615610	19.635968
52.164522	1512.032822	19.640986
51.856673	1533.765395	19.646003
52.114628	1515.803945	19.651021
52.079442	1511.428207	19.656039
51.976291	1517.023118	19.661056
52.194208	1511.865896	19.666074
52.581322	1506.236291	19.671091
52.202444	1505.731375	19.676109
52.456017	1514.031117	19.681127
52.253118	1497.830448	19.686144
52.379250	1497.100959	19.691162
52.315525	1521.766963	19.696179
52.128083	1502.565929	19.701197
52.530921	1526.392943	19.706215
52.384256	1541.765336	19.711232
52.808212	1532.161488	19.716250
53.059342	1535.229900	19.721267
52.579024	1535.591823	19.726285
53.000568	1528.526406	19.731303
52.965017	1538.581574	19.736320
53.260376	1537.971932	19.741338
53.239426	1533.242507	19.746355
53.233491	1541.817399	19.751373
53.723972	1527.458145	19.756391
53.303604	1534.296062	19.761408
53.454515	1531.438758	19.766426
53.593235	1538.118157	19.771443
53.473009	1525.872730	19.776461
53.339557	1529.040908	19.781479
53.012779	1533.026553	19.786496
53.339691	1533.903811	19.791514
53.062653	1534.315989	19.796531
53.271883	1545.673831	19.801549
53.733480	1554.977265	19.806567
53.780184	1552.553458	19.811584
54.245751	1549.942146	19.816602
54.032753	1560.524809	19.821619
54.504408	1557.942603	19.826637
54.419705	1548.347612	19.831655
54.417617	1561.781047	19.836672
54.379341	1547.569575	19.841690
53.825136	1531.771558	19.846707
53.874398	1545.094538	19.851725
54.380117	1543.384339	19.856743
54.455527	1552.186903	19.861760
54.353246	1568.107816	19.866778
54.481501	1554.590766	19.871795
54.379056	1549.064285	19.876813
54.509795	1552.681853	19.881831
54.370311	1556.213778	19.886848
54.116380	1548.891519	19.891866
54.359635	1561.184367	19.896883
54.224732	1562.720931	19.901901
54.848622	1566.384355	19.906919
54.675077	1583.394274	19.911936
55.087380	1579.649985	19.916954
54.823229	1575.846243	19.921971
54.874498	1578.789248	19.926989
55.357789	1567.674598	19.932007
55.070432	1578.610656	19.937024
55.359536	1573.284388	19.942042
55.151900	1565.052824	19.947059
55.364694	1572.131751	19.952077
55.460437	1568.153398	19.957095
55.524414	1571.624544	19.962112
55.476790	1572.852435	19.967130
55.481831	1574.846714	19.972147
55.351597	1576.485840	19.977165
55.358707	1566.731198	19.982183
54.979829	1572.119759	19.987200
55.407676	1591.089079	19.992218
55.677904	1595.379575	19.997235
55.609427	1597.729856	20.002253
56.051867	1595.708499	20.007271
55.699728	1598.867756	20.012288
56.093534	1600.817675	20.017306
55.627465	1594.733042	20.022323
55.528482	1604.220467	20.027341
55.972590	1604.136759	20.032359
56.031030	1632.269879	20.037376
56.710303	1630.519969	20.042394
56.711829	1628.268752	20.047411
56.530947	1625.284590	20.052429
56.855735	1617.585012	20.057447
56.738144	1603.575742	20.062464
56.245836	1590.500925	20.067482
56.876845	1602.692925	20.072499
56.408099	1603.053134	20.077517
56.554479	1605.150225	20.082535
56.556842	1622.528899	20.087552
56.803640	1615.101427	20.092570
57.011521	1612.237844	20.097587
56.417554	1626.521401	20.102605
56.782548	1620.120318	20.107623
56.894853	1620.083960	20.112640
56.784571	1628.024262	20.117658
56.981468	1629.360354	20.122675
57.128297	1651.357677	20.127693
57.294472	1643.724842	20.132711
57.522965	1648.716645	20.137728
57.422842	1661.047223	20.142746
57.748959	1645.433300	20.147763
57.642816	1645.028566	20.152781
57.594855	1642.137775	20.157799
57.443687	1647.255693	20.162816
57.618155	1663.431524	20.167834
57.506022	1642.428735	20.172851
57.570043	1648.706605	20.177869
58.028333	1645.649491	20.182887
57.920664	1650.905084	20.187904
57.795485	1638.661370	20.192922
57.987375	1654.605012	20.197939
58.047820	1666.140658	20.202957
58.223182	1658.628329	20.207975
58.125557	1663.662218	20.212992
58.322019	1650.823092	20.218010
58.618357	1658.633824	20.223027
58.310764	1662.253781	20.228045
58.418059	1649.550044	20.233063
58.485245	1664.433344	20.238080
58.252494	1659.311573	20.243098
58.793397	1644.514211	20.248115
58.737597	1656.532974	20.253133
58.469582	1660.808508	20.258151
58.633394	1647.345533	20.263168
58.543847	1655.932927	20.268186
58.848936	1668.674244	20.273203
58.776443	1674.555053	20.278221
59.041539	1685.034589	20.283239
58.829627	1685.508440	20.288256
59.115020	1680.550614	20.293274
59.256278	1690.571350	20.298291
58.846292	1689.157316	20.303309
59.084221	1677.143687	20.308327
59.163164	1690.805939	20.313344
59.106541	1686.202424	20.318362
59.059421	1694.321865	20.323379
59.257012	1717.263921	20.328397
59.598661	1706.678417	20.333415
59.669796	1710.954017	20.338432
59.859318	1715.012245	20.343450
59.864272	1707.886076	20.348467
59.612487	1713.892774	20.353485
59.620207	1717.252792	20.358503
60.003781	1701.216576	20.363520
59.615270	1710.016374	20.368538
60.068140	1717.573937	20.373555
59.762922	1735.299984	20.378573
59.928609	1731.281098	20.383591
60.260684	1743.021884	20.388608
60.225897	1732.931387	20.393626
60.643935	1733.919174	20.398643
60.546068	1740.275204	20.403661
60.889470	1733.101165	20.408679
60.821424	1740.539924	20.413696
60.591442	1738.714299	20.418714
60.739806	1723.294413	20.423731
60.799359	1730.759517	20.428749
60.830492	1733.903492	20.433767
60.889284	1729.917622	20.438784
60.623592	1733.700138	20.443802
61.129543	1728.798752	20.448819
61.064376	1727.247036	20.453837
60.860127	1727.434619	20.458855
60.896392	1726.949467	20.463872
61.031896	1744.255300	20.468890
61.085069	1754.368576	20.473907
61.053397	1771.946326	20.478925
61.073055	1754.026535	20.483943
61.347997	1757.251078	20.488960
61.265205	1757.358362	20.493978
61.811378	1749.429246	20.498995
61.494284	1754.991692	20.504013
61.802334	1773.464564	20.509031
62.000947	1774.920252	20.514048
61.903308	1784.599274	20.519066
62.330980	1767.805401	20.524083
61.962458	1779.016594	20.529101
62.143579	1775.067775	20.534119
62.503354	1763.989731	20.539136
62.308922	1756.957306	20.544154
62.600991	1739.180683	20.549171
62.367384	1733.750997	20.554189
62.120140	1741.007584	20.559207
61.994521	1750.803595	20.564224
62.361899	1766.016081	20.569242
62.291794	1766.521416	20.574259
62.572366	1776.534932	20.579277
62.372563	1767.589061	20.584295
62.527615	1764.052966	20.589312
62.521114	1779.707318	20.594330
62.670900	1766.601827	20.599347
62.797439	1787.441819	20.604365
62.813130	1793.243936	20.609383
62.907217	1790.185174	20.614400
62.949256	1798.661545	20.619418
62.887612	1801.504368	20.624435
62.941307	1794.395102	20.629453
63.038392	1804.023654	20.634471
63.153952	1795.871023	20.639488
63.011640	1796.816584	20.644506
63.320062	1798.776112	20.649523
63.383784	1819.709392	20.654541
63.679869	1826.322563	20.659559
63.690642	1825.216304	20.664576
63.712745	1827.206221	20.669594
63.927930	1806.747080	20.674611
64.020000	1818.392365	20.679629
64.113679	1815.314573	20.684647
64.248096	1815.445800	20.689664
63.953642	1818.925056	20.694682
63.817020	1814.120772	20.699699
63.932213	1820.244998	20.704717
63.892080	1821.446281	20.709735
64.165012	1813.045615	20.714752
64.294519	1818.860622	20.719770
64.180633	1818.374496	20.724787
64.067221	1831.848606	20.729805
64.081343	1843.218243	20.734823
64.278909	1839.564882	20.739840
64.571399	1844.448351	20.744858
64.657179	1840.256837	20.749875
64.450899	1845.427819	20.754893
64.634727	1845.518995	20.759911
65.201400	1854.248820	20.764928
65.098299	1861.511168	20.769946
65.449767	1854.892171	20.774963
65.576017	1856.549960	20.779981
65.121451	1840.654263	20.784999
65.026181	1837.009928	20.790016
64.807047	1857.668189	20.795034
65.272380	1857.370369	20.800051
65.472951	1850.760562	20.805069
65.178649	1862.303605	20.810087
65.446022	1862.647479	20.815104
65.537111	1860.145629	20.820122
65.488218	1860.259516	20.825139
65.159655	1863.245265	20.830157
65.550610	1892.842042	20.835175
65.960440	1887.778558	20.840192
65.847553	1895.350180	20.845210
66.216726	1899.400225	20.850227
66.245079	1889.845585	20.855245
66.152531	1895.955552	20.860263
66.346924	1894.400490	20.865280
66.246722	1886.261814	20.870298
66.049742	1884.199642	20.875315
66.347272	1890.226450	20.880333
66.467940	1908.320851	20.885351
67.181926	1913.388010	20.890368
66.694920	1902.603123	20.895386
66.762293	1889.767218	20.900403
67.100797	1890.829963	20.905421
66.901864	1885.344105	20.910439
66.540847	1882.776622	20.915456
66.961233	1901.130703	20.920474
67.028857	1912.005385	20.925491
67.142111	1907.989016	20.930509
67.536319	1912.083150	20.935527
67.290391	1920.843760	20.940544
67.225630	1921.705262	20.945562
67.037607	1919.791785	20.950579
67.472013	1919.935442	20.955597
67.667503	1917.519272	20.960615
67.625469	1915.694650	20.965632
67.398563	1920.683261	20.970650
67.430021	1914.083068	20.975667
67.425486	1913.196432	20.980685
67.476116	1915.041309	20.985703
67.568544	1923.115176	20.990720
68.047245	1937.992741	20.995738
67.943187	1939.842909	21.000755
68.218490	1943.176671	21.005773
67.706199	1936.076821	21.010791
68.146666	1942.834865	21.015808
67.871864	1936.949368	21.020826
67.898570	1921.595445	21.025843
68.143318	1935.006525	21.030861
68.512682	1964.779823	21.035879
68.749362	1963.453960	21.040896
68.944288	1958.224020	21.045914
68.557097	1958.613273	21.050931
69.002704	1959.819330	21.055949
68.943750	1948.692054	21.060967
69.111287	1952.573093	21.065984
68.865330	1966.799653	21.071002
69.048608	1953.052124	21.076019
69.223388	1954.097248	21.081037
69.028482	1965.001571	21.086055
69.378433	1950.482097	21.091072
69.434252	1959.939633	21.096090
69.140203	1964.069372	21.101107
69.365433	1956.002066	21.106125
69.149004	1964.098451	21.111143
69.050236	1968.462428	21.116160
69.447349	1975.181199	21.121178
69.545910	1983.696752	21.126195
70.037384	1979.708996	21.131213
69.783678	1979.508735	21.136231
69.510191	1984.390903	21.141248
69.825220	1986.249572	21.146266
69.738167	1999.825958	21.151283
70.087067	2004.610206	21.156301
70.119075	2020.790664	21.161319
70.165779	2013.586203	21.166336
70.464474	2015.466470	21.171354
70.879498	2006.219869	21.176371
70.960494	2000.348183	21.181389
70.592465	2007.911830	21.186407
70.789295	2001.395480	21.191424
70.856382	2001.759661	21.196442
70.898307	2007.222521	21.201459
70.885248	1997.233563	21.206477
70.660471	2004.254302	21.211495
70.847729	1991.340635	21.216512
70.991348	2001.948127	21.221530
70.814962	2008.721922	21.226547
70.750758	1996.451706	21.231565
70.804636	2020.658771	21.236583
71.013058	2014.926635	21.241600
71.281679	2016.106634	21.246618
71.400955	2021.637023	21.251635
71.171762	2020.669605	21.256653
71.338487	2031.847449	21.261671
71.801968	2058.953105	21.266688
72.091924	2052.698678	21.271706
71.760040	2058.304419	21.276723
72.587345	2053.013646	21.281741
72.438855	2049.108792	21.286759
72.453848	2026.293128	21.291776
72.253278	2019.607228	21.296794
72.058985	2008.677057	21.301811
72.192709	2015.133695	21.306829
72.404321	2039.033061	21.311847
72.457953	2031.544012	21.316864
72.485941	2028.767554	21.321882
72.150589	2037.233000	21.326899
72.752303	2032.316287	21.331917
72.233291	2023.571816	21.336935
71.987124	2030.611455	21.341952
72.316350	2042.716289	21.346970
72.776962	2049.603322	21.351987
72.981153	2054.753194	21.357005
73.117432	2060.369558	21.362023
73.164819	2059.152714	21.367040
73.079657	2058.852758	21.372058
72.973124	2061.416857	21.377075
72.919095	2065.319972	21.382093
73.188072	2077.771565	21.387111
73.113653	2078.266994	21.392128
73.706322	2083.230451	21.397146
73.462995	2095.376203	21.402163
73.604745	2097.331820	21.407181
73.602260	2092.222635	21.412199
73.406378	2098.535172	21.417216
73.835417	2098.061476	21.422234
73.778661	2102.426224	21.427251
74.307801	2103.772017	21.432269
74.232504	2111.179676	21.437287
74.500174	2105.511725	21.442304
74.706374	2114.481956	21.447322
74.900729	2112.999706	21.452339
74.758358	2075.248522	21.457357
74.598481	2078.221987	21.462375
74.490782	2082.232390	21.467392
74.625985	2093.151146	21.472410
74.497416	2100.382779	21.477427
74.592224	2098.793764	21.482445
74.626735	2105.757925	21.487463
74.459404	2110.772181	21.492480
74.714156	2104.892608	21.497498
74.762575	2125.724907	21.502515
75.060758	2122.808123	21.507533
75.351433	2131.427431	21.512551
75.106593	2129.269405	21.517568
75.382326	2129.574311	21.522586
75.207884	2137.702821	21.527603
75.627594	2131.586945	21.532621
75.624590	2136.357936	21.537639
75.720184	2147.939705	21.542656
75.867090	2150.541853	21.547674
75.933645	2157.138967	21.552691
75.960339	2154.887254	21.557709
76.245218	2152.665704	21.562727
76.168301	2157.420965	21.567744
76.503920	2151.874433	21.572762
76.525782	2151.360353	21.577779
76.329182	2146.948514	21.582797
76.674378	2139.497052	21.587815
76.469522	2149.988428	21.592832
76.810132	2145.177417	21.597850
76.709548	2142.073597	21.602867
76.567315	2149.902726	21.607885
76.728661	2142.274380	21.612903
76.682769	2149.803367	21.617920
76.757426	2141.572084	21.622938
76.720793	2153.579801	21.627955
76.871873	2168.687301	21.632973
77.166444	2177.151282	21.637991
76.859610	2178.453547	21.643008
77.356806	2188.006776	21.648026
77.054872	2182.840361	21.653043
77.271647	2173.718143	21.658061
77.290649	2178.493974	21.663079
77.539653	2169.044614	21.668096
77.594564	2173.182093	21.673114
78.071687	2191.134074	21.678131
78.193436	2192.605457	21.683149
77.912894	2202.571829	21.688167
77.857465	2197.267048	21.693184
78.016703	2196.823170	21.698202
78.517175	2193.599351	21.703219
78.256213	2195.757536	21.708237
78.317483	2201.907555	21.713255
78.467921	2196.609696	21.718272
78.598091	2193.937768	21.723290
78.396531	2201.028374	21.728307
78.602589	2193.945513	21.733325
78.385210	2186.710994	21.738343
78.260663	2205.554660	21.743360
78.704240	2211.631668	21.748378
78.489000	2215.036314	21.753395
78.767488	2214.047584	21.758413
79.232855	2218.065285	21.763431
78.887980	2220.517628	21.768448
79.358207	2208.875005	21.773466
78.950899	2221.038701	21.778483
79.272298	2228.110615	21.783501
79.228437	2233.358224	21.788519
79.495836	2240.558150	21.793536
79.702215	2236.660743	21.798554
79.557946	2236.082585	21.803571
79.978029	2235.639497	21.808589
79.716435	2244.496177	21.813607
79.834732	2252.796039	21.818624
80.082679	2238.730905	21.823642
80.238727	2261.950297	21.828659
80.458229	2270.083066	21.833677
80.582134	2270.205996	21.838695
80.292133	2273.118330	21.843712
80.656916	2267.752551	21.848730
80.577924	2263.203736	21.853747
80.526056	2271.807292	21.858765
80.961979	2254.228530	21.863783
80.841104	2267.665478	21.868800
80.687841	2260.929534	21.873818
80.970774	2263.581854	21.878835
80.737370	2258.763111	21.883853
81.215512	2256.516304	21.888871
81.036950	2259.550562	21.893888
81.010481	2255.519006	21.898906
81.148375	2272.739614	21.903923
81.371388	2284.807668	21.908941
81.598880	2289.134356	21.913959
81.564232	2293.345125	21.918976
81.482328	2289.060539	21.923994
81.429576	2289.111292	21.929011
81.409178	2289.283065	21.934029
82.010301	2296.001729	21.939047
82.230298	2307.216833	21.944064
81.945100	2316.090445	21.949082
82.362268	2303.798310	21.954099
82.472295	2310.909914	21.959117
82.581989	2310.067957	21.964135
82.329240	2313.016856	21.969152
82.458845	2306.579394	21.974170
82.257253	2308.922845	21.979187
82.168391	2308.159364	21.984205
82.480832	2309.985433	21.989223
82.580002	2315.196838	21.994240
82.693849	2328.806058	21.999258
82.911110	2336.190676	22.004275
83.058693	2335.543226	22.009293
83.241329	2330.290981	22.014311
82.946896	2341.506478	22.019328
82.974739	2338.313292	22.024346
82.935891	2327.826260	22.029363
83.171239	2343.229428	22.034381
83.723400	2354.575096	22.039399
83.278713	2367.831407	22.044416
83.573534	2363.488683	22.049434
83.584413	2353.609308	22.054451
83.401363	2355.141702	22.059469
83.855535	2359.865167	22.064487
84.000675	2363.717535	22.069504
84.041461	2379.686504	22.074522
84.479860	2382.302920	22.079539
84.349972	2385.618506	22.084557
84.355101	2379.024433	22.089575
84.429371	2383.831546	22.094592
84.542888	2382.146112	22.099610
84.311421	2383.799294	22.104627
84.135795	2378.070846	22.109645
84.591009	2386.165316	22.114663
84.674316	2393.873056	22.119680
84.775619	2411.811222	22.124698
84.940643	2416.651770	22.129715
84.944150	2413.792090	22.134733
85.156169	2412.050616	22.139751
85.072264	2419.251987	22.144768
85.433276	2433.974890	22.149786
85.722024	2437.722647	22.154803
85.948891	2442.047907	22.159821
85.980442	2433.395871	22.164839
85.921066	2428.003087	22.169856
85.933084	2431.554070	22.174874
85.945698	2428.298820	22.179891
86.173298	2439.013002	22.184909
86.358914	2433.398449	22.189927
86.225457	2425.843281	22.194944
86.286551	2434.658557	22.199962
86.305953	2433.884266	22.204979
86.089753	2431.548446	22.209997
86.030803	2432.211000	22.215015
86.307754	2439.794055	22.220032
86.850798	2449.651264	22.225050
86.775245	2446.907586	22.230067
86.811057	2463.393564	22.235085
86.941708	2456.014998	22.240103
86.975302	2463.573913	22.245120
87.274976	2453.006254	22.250138
87.406482	2451.830791	22.255155
87.686067	2459.414011	22.260173
87.504451	2451.587874	22.265191
87.469314	2448.400545	22.270208
87.371271	2448.459176	22.275226
87.706924	2457.254882	22.280243
87.445278	2454.683871	22.285261
87.546151	2464.182300	22.290279
87.579677	2480.940503	22.295296
87.522875	2484.889061	22.300314
87.830678	2472.376694	22.305331
87.885572	2486.597715	22.310349
88.382976	2501.788461	22.315367
88.331199	2506.421967	22.320384
88.170961	2510.561626	22.325402
88.566227	2504.510663	22.330419
88.450878	2506.694431	22.335437
88.734102	2513.076185	22.340455
88.898150	2506.157198	22.345472
88.718351	2504.671388	22.350490
88.640653	2501.347195	22.355507
88.403766	2507.054909	22.360525
88.963837	2515.537406	22.365543
88.945502	2538.112853	22.370560
88.827460	2542.621503	22.375578
89.200017	2528.537091	22.380595
89.314448	2540.789811	22.385613
89.098058	2540.490861	22.390631
89.174096	2557.301369	22.395648
89.564808	2562.461731	22.400666
89.591627	2554.758174	22.405683
89.596432	2572.270183	22.410701
89.965396	2566.345187	22.415719
90.221318	2580.747234	22.420736
90.346835	2593.755590	22.425754
90.691455	2578.444340	22.430771
90.527372	2592.713060	22.435789
90.610065	2582.687233	22.440807
90.842615	2580.166813	22.445824
90.511022	2586.712194	22.450842
90.886200	2577.917082	22.455859
90.504014	2587.878254	22.460877
91.069789	2592.515836	22.465895
90.960033	2581.913980	22.470912
90.649229	2580.258289	22.475930
91.010003	2578.607365	22.480947
91.040597	2605.552855	22.485965
91.169157	2599.432942	22.490983
91.431674	2610.706197	22.496000
91.243737	2605.590088	22.501018
91.584131	2605.617804	22.506035
91.252155	2620.880366	22.511053
91.426598	2628.851884	22.516071
91.920568	2632.348667	22.521088
91.763369	2644.963065	22.526106
91.974456	2633.795593	22.531123
92.304142	2622.126676	22.536141
92.634672	2629.763762	22.541159
92.489814	2636.922949	22.546176
92.463311	2633.258597	22.551194
92.813275	2641.767811	22.556211
92.859193	2660.497255	22.561229
93.230946	2651.312340	22.566247
93.177976	2651.847743	22.571264
92.687256	2647.850674	22.576282
93.284205	2653.613952	22.581299
93.221056	2661.753085	22.586317
93.107195	2655.773988	22.591335
93.200802	2648.681158	22.596352
93.246015	2657.946006	22.601370
93.282682	2649.522910	22.606387
93.245972	2659.886853	22.611405
93.892244	2672.142143	22.616423
93.949792	2670.218699	22.621440
93.938929	2680.514609	22.626458
94.213524	2673.814864	22.631475
93.897458	2673.898893	22.636493
93.957124	2684.244171	22.641511
94.003151	2665.309188	22.646528
94.009522	2676.461837	22.651546
94.044479	2678.926087	22.656563
93.980500	2697.737314	22.661581
94.128989	2702.592102	22.666599
94.497983	2703.018610	22.671616
94.338257	2707.329878	22.676634
94.858775	2716.730381	22.681651
94.669836	2728.444047	22.686669
95.002665	2726.861304	22.691687
95.530574	2729.215762	22.696704
95.035293	2727.490740	22.701722
95.465468	2733.515844	22.706739
95.595826	2730.261152	22.711757
95.560037	2728.379500	22.716775
95.576349	2721.436801	22.721792
95.594778	2720.701630	22.726810
95.761074	2718.365353	22.731827
95.950758	2746.974459	22.736845
96.346064	2748.868971	22.741863
96.541238	2758.149648	22.746880
96.461420	2756.756341	22.751898
96.179592	2754.265381	22.756915
96.421547	2751.706768	22.761933
96.557721	2762.140827	22.766951
96.683889	2744.809336	22.771968
96.397071	2749.879368	22.776986
96.453087	2753.149155	22.782003
96.907090	2754.353696	22.787021
96.732510	2762.977802	22.792039
96.738088	2772.298084	22.797056
96.886764	2774.002265	22.802074
97.046172	2775.881827	22.807091
97.367825	2769.696871	22.812109
96.971521	2770.388414	22.817127
97.479802	2798.821750	22.822144
97.272415	2807.046600	22.827162
97.464176	2805.385198	22.832179
97.846876	2813.299172	22.837197
97.651015	2818.103028	22.842215
98.310926	2821.686011	22.847232
98.107350	2824.455827	22.852250
98.185251	2835.577480	22.857267
98.054255	2838.322707	22.862285
97.884505	2831.487865	22.867303
98.367591	2837.781023	22.872320
98.726752	2851.363947	22.877338
99.049298	2854.521608	22.882355
99.205835	2862.668638	22.887373
99.273679	2853.285606	22.892391
99.355686	2857.708933	22.897408
99.411711	2857.297840	22.902426
99.501295	2842.900078	22.907443
99.469325	2849.432671	22.912461
99.322626	2854.745316	22.917479
99.778772	2837.552886	22.922496
99.565900	2848.818654	22.927514
99.527544	2859.920561	22.932531
99.735840	2850.284414	22.937549
99.526891	2854.329856	22.942567
99.773981	2864.583068	22.947584
99.944111	2868.252112	22.952602
100.114020	2873.533705	22.957619
100.202077	2884.749380	22.962637
99.883214	2879.639460	22.967655
100.453788	2890.456920	22.972672
100.183091	2909.548022	22.977690
100.572968	2899.257857	22.982707
101.009757	2896.879220	22.987725
100.732528	2897.939654	22.992743
101.280536	2889.974819	22.997760
101.281451	2904.607092	23.002778
101.607247	2907.953982	23.007795
101.613018	2903.898229	23.012813
101.080194	2906.050844	23.017831
101.467347	2904.040232	23.022848
101.547558	2927.622746	23.027866
101.440476	2934.182746	23.032883
101.602455	2922.758627	23.037901
101.733037	2917.575216	23.042919
101.669974	2921.908365	23.047936
101.616500	2941.393905	23.052954
102.104351	2940.005200	23.057971
102.283631	2951.356236	23.062989
101.673593	2953.369262	23.068007
102.339845	2958.540524	23.073024
102.616186	2974.109194	23.078042
102.777034	2961.367185	23.083059
102.995033	2970.067475	23.088077
103.292190	2968.619731	23.093095
103.681698	2968.314940	23.098112
103.237982	2971.564205	23.103130
103.292583	2964.057223	23.108147
103.640157	2967.286753	23.113165
103.329242	2970.549505	23.118183
103.568057	2960.955883	23.123200
103.634614	2962.781523	23.128218
103.467530	2967.537365	23.133235
103.938668	2976.957211	23.138253
104.087527	2997.223524	23.143271
104.107422	2994.107890	23.148288
104.120748	2985.786495	23.153306
104.154120	2998.476969	23.158323
104.388956	2991.722046	23.163341
104.068688	2997.185461	23.168359
104.224023	2997.427216	23.173376
104.815385	3010.921520	23.178394
104.862082	3007.890034	23.183411
105.152933	3007.225183	23.188429
104.795672	3017.353173	23.193447
104.935142	3003.653681	23.198464
104.960489	3009.830823	23.203482
105.141757	3022.166184	23.208499
105.146903	3028.312421	23.213517
105.267970	3038.667672	23.218535
105.619141	3032.782052	23.223552
105.925791	3043.608588	23.228570
105.797822	3055.482103	23.233587
106.034114	3067.269848	23.238605
105.946598	3061.255533	23.243623
106.371667	3055.909640	23.248640
106.321377	3066.739269	23.253658
106.106974	3056.535465	23.258675
106.858617	3060.336410	23.263693
106.654825	3066.129014	23.268711
106.414838	3057.186473	23.273728
106.806951	3083.584496	23.278746
107.009054	3093.078395	23.283763
107.093147	3092.591795	23.288781
107.128508	3095.565868	23.293799
107.215604	3093.880786	23.298816
107.334528	3091.686528	23.303834
107.283333	3097.183467	23.308851
107.396339	3098.210927	23.313869
107.447020	3123.135575	23.318887
107.655028	3112.831621	23.323904
107.789876	3121.299682	23.328922
108.010172	3130.837447	23.333939
108.230968	3117.117724	23.338957
108.100668	3133.316719	23.343975
107.898640	3143.456539	23.348992
108.698447	3148.021174	23.354010
108.337936	3146.465558	23.359027
108.967857	3148.156400	23.364045
108.405572	3151.027670	23.369063
108.904872	3144.767545	23.374080
108.761849	3138.912760	23.379098
108.710159	3148.670669	23.384115
109.090518	3150.437786	23.389133
109.140368	3154.758641	23.394151
109.252835	3160.114783	23.399168
109.333725	3170.706674	23.404186
109.367657	3167.549318	23.409203
109.638564	3170.145125	23.414221
109.516625	3192.984701	23.419239
109.695175	3196.198904	23.424256
110.012769	3190.615221	23.429274
109.841768	3200.179892	23.434291
110.311738	3198.310277	23.439309
109.839212	3216.142628	23.444327
110.260384	3206.821468	23.449344
110.751760	3210.661127	23.454362
110.653624	3225.043543	23.459379
110.811831	3202.589868	23.464397
110.775862	3224.114933	23.469415
111.079068	3231.556447	23.474432
111.289598	3236.428315	23.479450
111.254697	3242.610782	23.484467
111.646178	3235.832625	23.489485
111.826776	3234.990320	23.494503
111.827568	3235.767049	23.499520
112.154359	3231.572735	23.504538
111.678263	3232.464089	23.509555
112.224867	3221.093122	23.514573
111.965056	3234.036164	23.519591
112.199389	3236.359295	23.524608
112.568879	3230.986307	23.529626
112.168280	3245.313605	23.534643
112.424572	3251.229067	23.539661
112.499795	3262.910116	23.544679
112.706614	3264.470495	23.549696
112.820189	3261.449956	23.554714
112.570431	3268.255713	23.559731
112.622187	3264.583201	23.564749
113.053198	3285.848517	23.569767
113.015233	3289.332368	23.574784
113.184631	3288.865129	23.579802
113.821585	3289.820987	23.584819
114.107585	3292.380858	23.589837
114.122114	3285.109469	23.594855
114.210933	3289.116844	23.599872
114.124074	3287.048686	23.604890
114.319697	3297.437065	23.609907
114.565286	3297.391083	23.614925
114.619447	3299.812103	23.619943
114.797266	3306.855486	23.624960
114.881602	3296.112409	23.629978
114.725868	3298.656298	23.634995
114.859680	3291.945103	23.640013
114.704596	3303.079607	23.645031
114.235919	3292.238940	23.650048
114.747763	3299.077917	23.655066
114.849597	3330.124996	23.660083
114.813249	3325.732794	23.665101
115.037057	3330.441479	23.670119
114.947729	3360.519442	23.675136
115.158922	3350.191972	23.680154
115.438077	3358.018615	23.685171
115.516288	3381.132475	23.690189
115.757586	3384.560360	23.695207
115.990519	3393.159604	23.700224
116.418468	3382.691179	23.705242
116.108181	3381.457155	23.710259
116.277355	3381.812769	23.715277
116.390699	3402.284689	23.720295
116.456969	3415.085420	23.725312
116.269520	3412.856310	23.730330
116.590185	3423.862683	23.735347
117.058803	3422.155863	23.740365
117.031642	3443.101045	23.745383
117.298596	3444.842449	23.750400
117.595179	3437.919653	23.755418
116.963651	3447.353488	23.760435
117.310182	3434.012703	23.765453
117.605699	3459.504511	23.770471
117.432788	3474.984537	23.775488
117.962766	3460.744532	23.780506
118.195633	3465.621050	23.785523
118.142261	3470.901161	23.790541
118.425121	3469.132511	23.795559
118.872373	3482.090814	23.800576
119.286139	3473.493151	23.805594
118.855468	3472.556172	23.810611
119.175706	3489.004709	23.815629
119.374667	3483.333833	23.820647
119.174644	3486.265380	23.825664
119.340846	3488.416739	23.830682
119.308207	3493.562725	23.835699
119.369654	3480.956005	23.840717
119.158620	3484.613377	23.845735
119.190007	3489.782246	23.850752
119.551734	3506.728271	23.855770
119.493660	3524.559419	23.860787
119.566605	3514.001537	23.865805
120.101921	3525.677231	23.870823
120.129542	3547.087118	23.875840
120.166865	3539.752003	23.880858
120.165375	3543.666493	23.885875
120.380842	3555.120259	23.890893
120.413852	3551.925576	23.895911
120.547952	3571.118317	23.900928
120.756237	3568.717890	23.905946
120.744480	3567.279799	23.910963
120.562054	3592.702770	23.915981
120.965166	3593.072489	23.920999
120.892342	3600.692457	23.926016
121.314130	3613.142876	23.931034
121.525624	3623.916251	23.936051
121.926875	3623.437071	23.941069
122.370131	3625.548181	23.946087
122.175642	3629.027263	23.951104
122.342875	3607.754971	23.956122
122.755626	3624.009233	23.961139
122.984502	3638.292721	23.966157
122.825586	3615.962110	23.971175
123.198739	3605.232907	23.976192
122.956169	3615.329734	23.981210
123.268224	3621.367227	23.986227
122.989579	3644.307769	23.991245
123.073017	3650.251552	23.996263
123.479695	3640.917175	24.001280
123.413703	3645.845889	24.006298
123.100252	3648.587942	24.011315
123.095586	3651.249052	24.016333
123.708973	3660.201326	24.021351
123.687726	3682.080103	24.026368
123.702597	3669.982894	24.031386
123.916989	3684.508188	24.036403
124.469313	3702.035925	24.041421
124.315863	3694.562967	24.046439
124.108169	3708.949366	24.051456
124.801062	3701.022386	24.056474
125.014521	3696.056517	24.061491
124.741982	3707.347332	24.066509
125.140533	3694.532768	24.071527
124.924609	3699.681943	24.076544
125.003425	3716.780850	24.081562
125.398057	3716.767722	24.086579
125.226640	3723.907190	24.091597
125.443109	3727.469176	24.096615
125.445864	3731.654273	24.101632
125.894655	3745.820814	24.106650
126.126312	3753.343301	24.111667
125.966895	3752.992980	24.116685
126.366996	3754.591947	24.121703
126.338578	3756.693611	24.126720
126.521972	3754.031913	24.131738
126.872934	3766.565420	24.136755
126.834826	3767.069468	24.141773
127.201577	3780.418097	24.146791
127.103324	3780.919091	24.151808
127.144611	3769.973744	24.156826
127.399940	3774.031685	24.161843
127.272671	3776.841028	24.166861
127.370716	3778.212347	24.171879
127.640927	3799.941555	24.176896
127.682743	3806.549368	24.181914
128.071308	3795.148980	24.186931
128.075121	3807.945788	24.191949
127.992472	3796.295306	24.196967
128.075698	3812.618389	24.201984
128.466749	3822.350415	24.207002
128.535957	3825.280846	24.212019
128.209757	3838.866074	24.217037
128.565538	3838.357393	24.222055
128.650678	3857.208969	24.227072
128.813150	3857.205069	24.232090
128.981949	3859.743850	24.237107
128.742538	3869.509213	24.242125
129.310521	3883.287284	24.247143
129.378419	3886.925038	24.252160
129.539226	3892.797075	24.257178
129.805197	3902.122648	24.262195
129.932924	3914.385283	24.267213
130.356035	3921.353769	24.272231
130.310767	3913.871885	24.277248
130.657899	3910.514592	24.282266
130.298176	3907.852452	24.287283
130.194593	3917.703278	24.292301
130.840247	3921.536523	24.297319
130.542481	3948.213009	24.302336
130.915109	3940.540012	24.307354
131.282446	3944.078301	24.312371
131.423186	3964.874788	24.317389
131.766036	3968.966744	24.322407
131.811475	3966.893564	24.327424
131.910275	3969.519127	24.332442
131.931530	3966.582211	24.337459
131.703465	3975.591423	24.342477
132.099887	3964.909311	24.347495
131.827781	3960.843290	24.352512
132.020932	3982.831556	24.357530
132.384882	3987.354290	24.362547
132.346017	3989.002586	24.367565
132.577421	3987.825857	24.372583
132.629178	4020.710185	24.377600
132.425106	4022.253495	24.382618
132.765130	4019.616661	24.387635
132.868912	4033.368022	24.392653
133.211526	4034.789506	24.397671
133.210242	4052.916213	24.402688
133.236332	4057.337311	24.407706
133.704691	4043.482951	24.412723
133.918057	4061.658849	24.417741
134.089103	4074.208947	24.422759
134.123375	4072.298625	24.427776
134.277736	4073.577986	24.432794
134.656683	4068.314177	24.437811
134.714837	4072.835102	24.442829
134.811010	4050.236120	24.447847
135.068333	4071.240657	24.452864
134.928514	4090.980889	24.457882
134.888400	4094.042823	24.462899
134.823354	4101.681436	24.467917
135.352693	4093.439543	24.472935
135.388759	4107.645478	24.477952
135.490702	4123.387826	24.482970
135.987702	4119.776192	24.487987
135.772292	4123.169468	24.493005
136.057076	4115.977054	24.498023
135.947618	4122.753308	24.503040
136.197301	4137.301148	24.508058
136.494398	4144.652772	24.513075
136.347502	4159.472466	24.518093
136.471153	4149.985728	24.523111
136.474439	4173.159211	24.528128
136.241453	4182.272901	24.533146
136.750577	4184.714950	24.538163
136.577620	4216.515920	24.543181
136.656056	4224.782875	24.548199
137.409305	4240.402369	24.553216
137.545256	4243.405318	24.558234
138.032923	4239.260535	24.563251
137.978144	4242.354057	24.568269
138.414435	4252.209592	24.573287
138.406521	4266.335533	24.578304
138.633763	4269.401359	24.583322
138.813948	4266.834597	24.588339
138.945855	4273.892699	24.593357
139.103166	4268.634342	24.598375
139.430804	4270.420147	24.603392
138.740411	4260.384360	24.608410
138.971009	4271.295585	24.613427
139.235335	4300.055465	24.618445
139.687460	4295.340928	24.623463
139.433688	4299.231937	24.628480
139.631018	4304.525633	24.633498
139.862085	4313.451694	24.638515
140.035926	4326.245638	24.643533
139.887177	4325.353361	24.648551
140.453745	4332.553457	24.653568
140.510096	4344.117960	24.658586
141.035620	4353.334380	24.663603
140.731763	4354.099689	24.668621
140.728347	4345.130699	24.673639
141.436453	4338.038323	24.678656
141.098652	4347.137143	24.683674
141.461419	4344.065771	24.688691
141.533339	4361.250782	24.693709
141.728637	4365.638102	24.698727
141.959347	4375.107588	24.703744
141.989287	4372.741626	24.708762
142.295458	4368.433878	24.713779
141.839987	4378.327782	24.718797
142.037518	4379.970131	24.723815
142.241844	4394.782017	24.728832
142.220978	4403.951736	24.733850
142.528130	4398.318560	24.738867
142.294425	4412.498479	24.743885
142.724146	4417.002598	24.748903
142.950443	4426.936646	24.753920
142.931422	4434.748140	24.758938
143.393988	4441.204019	24.763955
143.350195	4459.413818	24.768973
143.379075	4459.610741	24.773991
143.775146	4465.941784	24.779008
143.732554	4475.467514	24.784026
144.014802	4488.418885	24.789043
144.145464	4482.363637	24.794061
144.211597	4487.249918	24.799079
144.761709	4482.693947	24.804096
144.503092	4510.672864	24.809114
144.779468	4502.355621	24.814131
144.926822	4511.712972	24.819149
145.060669	4507.537995	24.824167
145.645827	4513.892542	24.829184
145.592699	4527.729326	24.834202
145.725293	4517.952288	24.839219
145.364405	4537.277620	24.844237
145.647782	4527.292188	24.849255
145.813701	4532.943926	24.854272
145.926514	4561.598610	24.859290
146.263392	4553.394578	24.864307
146.700247	4553.488657	24.869325
146.335438	4566.141867	24.874343
146.603008	4568.458134	24.879360
147.014870	4580.883413	24.884378
146.910790	4591.951744	24.889395
146.940284	4599.519464	24.894413
147.155376	4611.595369	24.899431
147.594550	4620.150586	24.904448
147.536765	4624.921157	24.909466
147.840851	4622.671680	24.914483
148.366548	4641.877028	24.919501
148.188467	4642.958202	24.924519
148.285769	4632.864070	24.929536
148.526583	4651.301886	24.934554
148.702203	4638.908055	24.939571
148.615944	4652.502377	24.944589
148.851074	4670.932887	24.949607
149.147986	4673.330942	24.954624
149.298496	4669.772105	24.959642
149.602456	4672.666664	24.964659
149.330872	4671.917505	24.969677
149.229061	4679.864857	24.974695
149.689003	4693.515824	24.979712
149.866273	4710.866502	24.984730
149.955335	4695.062298	24.989747
150.067971	4712.654381	24.994765
150.014316	4732.077623	24.999783
150.413717	4726.683436	25.004800
150.815304	4735.695745	25.009818
150.771292	4747.530690	25.014835
151.247852	4742.235567	25.019853
151.669199	4747.968415	25.024871
151.905546	4740.938061	25.029888
152.006134	4745.662026	25.034906
152.119922	4735.972611	25.039923
151.845386	4737.454401	25.044941
151.611115	4746.727696	25.049959
152.272901	4726.721860	25.054976
152.221026	4738.657317	25.059994
152.200567	4744.656485	25.065011
152.391617	4742.568985	25.070029
152.210351	4770.336361	25.075047
152.546442	4766.057027	25.080064
152.522099	4773.151804	25.085082
152.623934	4786.999829	25.090099
152.811552	4804.001240	25.095117
152.556763	4818.660634	25.100135
152.925648	4833.013826	25.105152
152.660724	4846.905968	25.110170
152.807443	4858.355519	25.115187
152.916947	4870.959346	25.120205
153.166790	4878.760104	25.125223
153.671961	4893.815692	25.130240
153.836536	4916.361614	25.135258
154.036401	4920.873545	25.140275
154.716922	4937.145574	25.145293
154.722733	4964.157522	25.150311
154.986443	4949.674313	25.155328
155.059032	4960.429438	25.160346
155.191235	4972.325602	25.165363
155.733936	4976.339133	25.170381
155.925370	4991.714000	25.175399
155.910240	4999.055016	25.180416
156.208169	4989.715365	25.185434
156.123978	4978.461136	25.190451
156.299145	4995.656954	25.195469
156.263617	5002.937163	25.200487
156.601822	5000.574900	25.205504
156.542179	5014.701404	25.210522
156.682342	5028.905546	25.215539
157.365088	5037.830627	25.220557
156.997234	5046.922217	25.225575
157.462611	5034.652653	25.230592
157.540784	5046.844834	25.235610
157.503761	5073.948307	25.240627
158.287588	5065.252012	25.245645
158.202462	5065.949713	25.250663
158.218187	5060.540060	25.255680
158.149663	5073.595550	25.260698
158.514435	5088.772959	25.265715
158.967737	5089.857329	25.270733
158.596423	5096.043749	25.275751
158.810982	5100.970271	25.280768
158.948988	5116.528513	25.285786
158.759121	5125.392691	25.290803
159.343726	5127.870064	25.295821
159.162558	5156.277143	25.300839
159.804234	5149.865524	25.305856
159.497506	5155.886950	25.310874
159.590812	5184.420004	25.315891
160.300357	5184.526519	25.320909
160.342422	5191.888887	25.325927
160.364593	5198.902543	25.330944
160.568529	5207.794620	25.335962
160.933109	5200.922811	25.340979
161.664870	5216.702763	25.345997
161.288255	5242.247522	25.351015
161.535171	5235.346710	25.356032
161.612173	5252.987419	25.361050
161.354839	5246.740449	25.366067
161.874531	5241.269119	25.371085
161.982502	5266.422006	25.376103
162.185906	5257.287598	25.381120
162.371229	5262.936790	25.386138
162.192260	5269.490749	25.391155
162.688517	5274.147136	25.396173
162.906554	5305.099810	25.401191
163.053914	5307.130509	25.406208
163.065889	5292.240107	25.411226
163.116643	5300.644110	25.416243
163.252400	5313.071103	25.421261
163.414997	5317.717273	25.426279
163.670630	5331.297036	25.431296
163.255799	5332.366582	25.436314
163.428916	5353.639150	25.441331
163.869763	5351.105529	25.446349
163.650971	5379.202265	25.451367
163.966661	5366.598870	25.456384
164.757987	5402.457547	25.461402
164.840394	5418.936795	25.466419
165.179760	5414.523660	25.471437
165.040622	5416.116225	25.476455
165.103651	5421.406899	25.481472
165.306159	5440.614266	25.486490
165.461969	5447.723681	25.491507
165.851225	5447.858711	25.496525
165.928381	5465.748482	25.501543
166.103336	5476.578397	25.506560
166.315073	5474.938222	25.511578
166.577427	5491.750847	25.516595
166.991134	5508.321134	25.521613
167.183395	5501.072108	25.526631
168.050531	5492.812260	25.531648
168.135340	5472.289324	25.536666
168.387454	5478.121281	25.541683
168.474614	5481.654639	25.546701
168.078041	5475.476257	25.551719
168.269653	5480.546076	25.556736
168.641823	5481.355266	25.561754
168.591707	5476.891100	25.566771
168.914503	5473.009882	25.571789
169.217746	5482.632643	25.576807
168.684398	5473.281221	25.581824
168.850100	5487.757970	25.586842
169.077003	5509.600670	25.591859
169.063201	5496.568879	25.596877
168.713426	5527.239785	25.601895
168.969429	5544.261808	25.606912
168.864857	5540.090908	25.611930
168.938573	5577.724266	25.616947
169.361643	5598.475495	25.621965
169.424434	5607.003280	25.626983
169.617648	5621.942199	25.632000
170.164787	5645.483180	25.637018
170.372740	5665.070285	25.642035
170.987471	5671.771651	25.647053
170.964099	5685.052502	25.652071
171.044072	5692.293079	25.657088
171.486584	5691.578654	25.662106
171.688754	5715.300770	25.667123
172.381867	5713.082150	25.672141
172.213245	5723.737874	25.677159
172.425845	5727.348212	25.682176
172.413112	5714.452695	25.687194
172.756677	5730.040585	25.692212
173.078705	5727.335962	25.697229
172.936103	5750.451232	25.702247
173.343744	5749.736266	25.707264
173.470589	5755.564219	25.712282
173.251173	5757.930024	25.717300
173.575720	5752.845928	25.722317
173.773903	5760.422957	25.727335
173.698953	5777.936983	25.732352
173.845168	5770.702528	25.737370
174.009562	5793.075313	25.742388
174.259380	5803.517051	25.747405
174.394641	5801.704415	25.752423
174.546636	5817.482333	25.757440
174.798419	5828.299798	25.762458
174.667010	5832.059140	25.767476
174.792972	5840.504556	25.772493
174.798191	5857.082463	25.777511
175.180929	5861.379387	25.782528
175.438711	5880.671481	25.787546
175.706429	5903.587666	25.792564
176.004646	5893.064588	25.797581
176.217099	5913.667546	25.802599
176.522850	5929.887168	25.807616
176.774574	5917.171836	25.812634
176.654693	5930.282594	25.817652
176.799227	5944.117502	25.822669
177.115608	5948.223416	25.827687
177.094328	5954.824056	25.832704
177.561108	5963.979086	25.837722
177.632945	5991.375653	25.842740
177.622288	5989.700901	25.847757
178.158388	5982.753950	25.852775
178.256670	6007.280009	25.857792
178.896392	6012.239735	25.862810
178.649954	6016.103966	25.867828
178.765146	6016.446515	25.872845
179.007313	6035.778000	25.877863
178.796920	6044.577178	25.882880
179.038445	6060.410638	25.887898
179.337214	6069.495837	25.892916
179.863137	6079.892534	25.897933
179.777725	6085.315455	25.902951
179.914792	6102.326236	25.907968
180.375433	6099.243476	25.912986
180.248190	6117.437489	25.918004
180.564125	6115.046455	25.923021
180.655137	6127.121590	25.928039
180.948621	6134.958688	25.933056
181.175730	6125.224491	25.938074
181.185010	6161.672860	25.943092
181.248692	6162.792549	25.948109
181.502791	6179.057190	25.953127
181.740196	6194.434700	25.958144
182.329391	6195.985755	25.963162
182.202722	6189.840458	25.968180
182.355061	6219.316974	25.973197
182.786129	6225.608305	25.978215
182.972916	6218.059806	25.983232
183.094642	6229.420382	25.988250
182.967551	6239.558879	25.993268
183.400480	6242.235150	25.998285
183.513166	6249.253221	26.003303
183.498502	6259.716518	26.008320
183.768927	6278.552215	26.013338
183.968083	6279.563687	26.018356
184.070254	6294.691942	26.023373
184.456777	6313.242312	26.028391
184.582870	6318.786300	26.033408
184.808068	6329.036755	26.038426
184.693148	6339.413504	26.043444
185.206929	6343.005723	26.048461
185.781411	6341.323245	26.053479
185.628995	6366.521315	26.058496
185.983963	6362.000598	26.063514
185.601372	6370.815022	26.068532
186.076083	6371.981792	26.073549
186.652552	6391.880635	26.078567
186.375188	6402.511864	26.083584
186.933066	6396.454990	26.088602
186.894417	6402.548364	26.093620
187.211350	6394.032444	26.098637
187.177025	6411.295539	26.103655
186.999619	6430.288891	26.108672
187.526793	6426.372885	26.113690
187.608413	6443.104957	26.118708
187.806344	6456.198294	26.123725
188.048345	6459.996105	26.128743
187.737136	6485.501754	26.133760
188.364206	6485.419520	26.138778
188.703046	6501.990237	26.143796
188.212659	6515.104421	26.148813
188.613094	6516.262999	26.153831
189.031456	6526.823462	26.158848
189.477156	6543.063124	26.163866
189.631380	6542.871581	26.168884
189.679210	6549.492554	26.173901
189.851820	6563.594284	26.178919
190.318260	6582.420798	26.183936
190.466240	6568.222201	26.188954
190.523629	6582.075220	26.193972
190.438176	6595.855771	26.198989
190.964202	6602.636383	26.204007
190.934959	6621.937831	26.209024
191.599027	6632.553849	26.214042
191.956423	6638.424368	26.219060
191.850634	6647.570446	26.224077
192.226084	6650.355516	26.229095
192.171314	6671.930174	26.234112
192.456187	6676.400611	26.239130
192.745890	6670.680124	26.244148
192.435782	6689.715403	26.249165
193.165647	6694.849470	26.254183
193.059883	6708.268051	26.259200
193.368553	6710.214396	26.264218
193.116039	6710.479894	26.269236
192.977108	6727.689740	26.274253
193.566547	6739.468778	26.279271
193.524148	6761.778666	26.284288
194.151991	6776.364536	26.289306
194.123436	6779.773971	26.294324
194.372558	6804.568535	26.299341
195.031190	6807.795131	26.304359
194.878808	6827.022668	26.309376
195.063893	6827.979798	26.314394
195.567631	6836.459021	26.319412
195.604013	6851.807386	26.324429
195.760186	6855.857317	26.329447
195.889813	6873.942820	26.334464
196.362503	6877.099346	26.339482
196.793278	6881.174793	26.344500
196.696617	6900.277441	26.349517
196.867123	6905.444144	26.354535
197.185386	6905.640540	26.359552
197.319385	6921.893505	26.364570
197.604464	6931.334296	26.369588
197.525200	6945.951311	26.374605
197.870036	6945.483337	26.379623
197.916400	6957.364083	26.384640
197.895070	6963.717072	26.389658
197.761384	6978.882592	26.394676
197.969736	6989.776554	26.399693
198.637771	6999.534507	26.404711
199.052760	7020.672108	26.409728
199.239676	7020.298744	26.414746
199.651934	7027.215687	26.419764
199.661721	7051.405953	26.424781
200.127516	7050.495854	26.429799
200.124068	7059.930051	26.434816
199.981902	7052.176395	26.439834
200.198527	7053.893058	26.444852
200.347768	7079.309411	26.449869
200.461543	7075.594652	26.454887
200.847126	7098.183197	26.459904
200.961237	7110.245032	26.464922
200.786941	7112.211371	26.469940
201.121297	7138.011497	26.474957
201.410861	7133.802223	26.479975
202.056472	7157.437893	26.484992
201.580625	7177.683293	26.490010
201.878160	7178.161133	26.495028
202.348456	7194.072924	26.500045
202.490857	7200.954986	26.505063
202.836028	7226.022598	26.510080
202.863934	7239.685746	26.515098
203.254603	7230.465701	26.520116
203.440016	7258.083950	26.525133
204.090722	7268.744352	26.530151
204.368799	7270.769857	26.535168
204.711732	7258.357741	26.540186
204.814619	7281.362632	26.545204
204.851869	7295.399174	26.550221
204.966520	7294.033577	26.555239
205.079147	7297.810438	26.560256
205.147106	7307.153440	26.565274
205.760162	7314.351579	26.570292
205.475501	7331.041152	26.575309
205.983270	7324.519657	26.580327
205.803770	7344.263446	26.585344
206.081777	7357.894826	26.590362
206.304640	7365.661513	26.595380
206.298858	7376.716349	26.600397
206.764465	7388.414739	26.605415
206.791432	7407.492849	26.610432
207.037876	7418.971505	26.615450
207.222810	7429.120645	26.620468
207.474686	7446.740832	26.625485
207.832496	7471.994193	26.630503
207.832088	7473.790080	26.635520
208.185031	7490.930514	26.640538
208.277596	7512.334698	26.645556
208.449758	7514.051670	26.650573
208.953711	7530.092132	26.655591
209.295593	7538.129074	26.660608
209.553257	7529.259258	26.665626
209.566613	7559.062895	26.670644
210.041149	7564.910470	26.675661
210.294004	7569.715669	26.680679
210.245758	7581.239195	26.685696
210.339477	7593.071641	26.690714
210.657097	7590.448557	26.695732
210.594888	7615.463595	26.700749
210.849740	7628.422488	26.705767
211.183540	7640.088498	26.710784
211.151914	7658.684342	26.715802
211.764957	7668.970042	26.720820
211.929831	7684.609877	26.725837
212.221127	7681.477611	26.730855
212.183356	7694.055663	26.735872
212.315419	7723.960501	26.740890
212.561722	7718.259411	26.745908
212.567902	7735.303821	26.750925
213.061299	7752.187415	26.755943
213.185165	7755.391516	26.760960
213.334871	7775.810773	26.765978
213.576308	7787.067633	26.770996
213.812689	7793.209828	26.776013
213.874913	7805.977013	26.781031
214.077545	7818.704470	26.786048
214.352853	7836.287353	26.791066
214.725031	7838.358031	26.796084
214.704695	7861.725161	26.801101
214.941881	7878.626807	26.806119
215.307739	7876.541521	26.811136
215.475361	7908.303533	26.816154
215.646491	7927.404921	26.821172
215.695707	7929.863707	26.826189
216.122675	7946.331598	26.831207
216.193828	7954.035428	26.836224
216.098443	7984.283931	26.841242
216.665682	8000.602685	26.846260
216.816271	8010.907520	26.851277
216.947927	8018.120938	26.856295
217.777154	8035.111599	26.861312
217.899365	8052.645194	26.866330
218.058304	8058.445071	26.871348
218.239901	8072.550606	26.876365
218.598022	8068.945678	26.881383
218.947944	8099.801333	26.886400
218.642297	8102.425893	26.891418
219.373629	8103.754398	26.896436
219.331764	8123.332282	26.901453
219.658229	8131.286224	26.906471
220.028791	8140.614377	26.911488
219.951213	8165.117716	26.916506
220.671961	8160.774709	26.921524
220.875709	8170.706196	26.926541
221.402134	8185.492863	26.931559
221.326288	8175.273452	26.936576
221.120648	8195.635393	26.941594
221.534579	8198.822377	26.946612
221.674214	8209.282740	26.951629
221.472016	8219.000144	26.956647
221.734463	8238.682267	26.961664
222.251019	8248.624343	26.966682
222.427620	8265.037055	26.971700
222.398182	8290.377761	26.976717
222.742829	8298.098795	26.981735
222.724529	8310.555186	26.986752
222.669546	8336.434201	26.991770
223.460900	8344.100356	26.996788
223.852600	8351.596255	27.001805
223.844846	8378.255957	27.006823
224.358707	8378.398007	27.011840
224.906753	8405.796096	27.016858
225.259441	8404.855781	27.021876
225.327047	8401.331860	27.026893
225.550871	8420.138436	27.031911
225.808200	8430.816579	27.036928
225.932514	8437.349307	27.041946
226.280677	8438.476503	27.046964
226.337780	8447.514005	27.051981
226.110674	8468.613135	27.056999
226.248884	8464.789258	27.062016
226.683518	8488.049061	27.067034
226.832789	8498.768732	27.072052
227.015559	8513.667622	27.077069
227.186098	8534.002501	27.082087
227.526377	8550.113577	27.087104
227.427090	8569.019398	27.092122
228.074850	8578.696623	27.097140
228.206296	8602.213050	27.102157
227.966124	8611.963748	27.107175
228.439801	8619.511605	27.112192
228.854332	8642.577257	27.117210
228.981927	8658.035965	27.122228
229.512630	8668.456436	27.127245
229.491800	8677.239144	27.132263
230.024492	8673.948656	27.137280
229.831147	8682.214815	27.142298
230.421021	8702.637370	27.147316
230.755033	8720.909399	27.152333
230.417771	8727.323957	27.157351
230.870807	8732.620228	27.162368
231.031339	8754.710360	27.167386
231.028913	8774.734645	27.172404
231.520277	8783.126389	27.177421
231.577447	8812.825112	27.182439
232.052516	8815.565760	27.187456
232.301015	8840.757453	27.192474
232.516304	8856.540559	27.197492
232.882791	8865.219996	27.202509
232.884356	8871.532159	27.207527
233.449240	8890.229383	27.212544
233.376169	8909.014703	27.217562
233.752012	8920.610126	27.222580
233.864902	8942.702878	27.227597
233.973485	8943.375043	27.232615
234.675006	8962.027722	27.237632
234.832668	8979.527342	27.242650
234.963391	8988.017376	27.247668
235.673231	8999.501750	27.252685
235.417657	9005.583131	27.257703
236.079148	9014.944865	27.262720
236.336909	9034.258547	27.267738
236.453309	9038.740166	27.272756
236.584199	9056.401040	27.277773
236.864246	9067.981680	27.282791
237.132973	9066.528250	27.287808
237.308264	9087.506580	27.292826
237.524832	9103.916708	27.297844
237.887999	9109.817133	27.302861
237.792827	9111.301190	27.307879
238.179267	9124.102513	27.312896
238.547627	9156.314340	27.317914
238.458469	9150.601212	27.322932
239.083072	9159.816319	27.327949
239.230835	9180.822950	27.332967
239.537560	9184.249187	27.337984
239.534008	9205.821197	27.343002
239.458526	9214.521073	27.348020
239.471425	9234.964025	27.353037
240.035031	9252.119614	27.358055
240.428133	9277.673284	27.363072
240.567948	9290.282336	27.368090
240.648234	9303.808642	27.373108
241.027039	9324.996268	27.378125
241.087670	9351.854253	27.383143
241.479593	9359.553818	27.388160
241.809545	9391.358932	27.393178
242.029381	9405.223029	27.398196
242.451303	9415.706078	27.403213
242.883008	9438.837792	27.408231
243.157562	9443.743954	27.413248
243.397486	9457.997835	27.418266
243.598705	9465.895162	27.423284
243.789077	9472.978239	27.428301
244.145998	9473.509360	27.433319
244.368654	9498.118748	27.438336
244.229093	9510.474022	27.443354
244.462506	9513.353969	27.448372
244.971286	9536.623541	27.453389
244.672974	9553.295643	27.458407
244.619222	9551.747363	27.463424
245.110133	9583.245849	27.468442
245.570200	9611.170197	27.473460
245.967098	9614.224015	27.478477
246.362909	9628.509796	27.483495
246.809448	9641.639531	27.488512
247.077373	9637.114159	27.493530
246.972711	9666.224444	27.498548
247.244483	9675.835283	27.503565
247.431177	9675.879380	27.508583
247.413691	9687.260716	27.513600
248.055600	9703.047436	27.518618
248.114750	9725.605445	27.523636
248.537732	9735.625361	27.528653
248.607410	9753.412915	27.533671
248.976286	9761.561537	27.538688
249.120798	9786.549777	27.543706
249.181992	9814.796387	27.548724
249.718760	9830.661258	27.553741
249.855179	9827.664445	27.558759
249.953099	9855.049608	27.563776
250.429547	9871.591676	27.568794
250.250546	9897.857641	27.573812
250.950772	9906.280069	27.578829
251.012963	9925.830375	27.583847
251.321413	9937.536142	27.588864
251.579125	9952.170356	27.593882
252.114266	9984.405931	27.598900
252.140932	9995.332769	27.603917
252.192098	10012.261908	27.608935
252.722127	10015.512795	27.613952
253.366791	10036.899274	27.618970
253.527720	10056.826500	27.623988
253.570871	10073.441940	27.629005
253.667271	10087.801233	27.634023
254.239964	10091.900552	27.639040
254.481257	10115.286847	27.644058
254.178517	10135.449108	27.649076
254.940406	10153.328339	27.654093
255.093171	10172.210172	27.659111
255.328796	10183.261737	27.664128
255.816518	10204.947712	27.669146
255.684474	10220.435080	27.674164
256.521257	10225.633795	27.679181
256.185540	10250.713131	27.684199
256.547806	10251.493897	27.689216
256.790730	10264.107953	27.694234
257.086576	10293.810177	27.699252
257.454192	10300.063217	27.704269
257.788495	10319.735259	27.709287
257.916048	10342.161528	27.714304
258.416726	10347.422902	27.719322
258.689335	10365.538393	27.724340
258.853598	10379.941878	27.729357
258.980858	10383.965196	27.734375
259.166387	10404.483531	27.739392
259.427592	10422.787664	27.744410
259.299969	10446.585938	27.749428
259.839018	10456.808489	27.754445
260.292728	10486.603939	27.759463
260.506538	10498.295033	27.764480
260.939407	10507.917570	27.769498
261.245459	10526.161634	27.774516
261.548064	10548.510430	27.779533
261.384804	10556.021866	27.784551
261.624563	10566.254547	27.789568
262.015788	10579.080675	27.794586
261.821488	10597.842321	27.799604
262.184951	10618.390614	27.804621
262.240673	10639.124482	27.809639
262.397638	10653.251344	27.814656
263.043236	10688.615574	27.819674
263.102859	10709.668715	27.824692
263.689955	10712.440820	27.829709
264.191966	10743.024398	27.834727
264.158493	10755.144896	27.839744
264.245492	10764.271729	27.844762
264.257163	10795.844699	27.849780
264.890622	10812.075849	27.854797
265.068304	10819.735896	27.859815
265.576572	10841.802980	27.864832
265.722476	10870.777165	27.869850
265.850350	10883.621839	27.874868
266.355928	10901.302416	27.879885
266.788579	10926.453590	27.884903
266.998534	10935.055251	27.889920
267.395347	10954.129289	27.894938
267.912507	10980.944523	27.899956
267.978285	10985.487835	27.904973
267.992110	11007.090128	27.909991
268.064706	11028.936401	27.915008
268.507062	11036.034474	27.920026
268.701104	11070.985737	27.925044
269.163353	11069.351271	27.930061
269.543043	11095.050295	27.935079
269.897143	11117.671037	27.940096
270.378910	11126.402779	27.945114
270.653416	11138.478987	27.950132
271.090701	11140.013909	27.955149
270.982803	11163.624861	27.960167
271.217623	11162.992983	27.965184
271.649047	11179.640745	27.970202
271.634682	11216.321260	27.975220
271.713037	11225.451359	27.980237
272.255034	11241.012691	27.985255
272.344137	11260.694892	27.990272
272.844700	11267.795268	27.995290
272.759685	11305.772527	28.000308
273.329446	11325.597550	28.005325
273.659903	11328.943919	28.010343
273.816445	11346.923717	28.015360
274.175099	11360.582238	28.020378
274.209401	11382.150929	28.025396
274.259591	11395.939221	28.030413
274.847716	11423.090098	28.035431
275.017531	11446.679217	28.040448
275.646627	11467.507709	28.045466
275.668062	11491.000088	28.050484
276.221904	11506.685769	28.055501
276.014705	11530.271912	28.060519
276.248210	11546.179143	28.065536
276.837088	11561.018514	28.070554
277.001365	11595.717442	28.075572
277.533723	11608.499810	28.080589
277.691874	11627.880356	28.085607
277.963984	11655.587238	28.090624
278.889644	11646.105322	28.095642
279.135554	11657.280679	28.100660
279.463410	11659.794058	28.105677
279.567203	11669.046254	28.110695
279.440622	11691.565240	28.115712
279.769129	11694.370003	28.120730
279.935842	11728.577228	28.125748
280.078800	11738.234226	28.130765
280.305825	11763.330090	28.135783
280.561629	11791.469253	28.140800
280.939815	11786.419294	28.145818
280.813819	11813.480833	28.150836
280.797566	11825.706436	28.155853
281.054495	11849.106861	28.160871
281.835300	11886.279900	28.165888
282.160795	11907.713741	28.170906
282.197025	11927.641049	28.175924
282.526917	11943.212110	28.180941
283.096310	11970.515906	28.185959
282.968123	11996.422391	28.190976
283.363148	12006.124566	28.195994
283.681967	12037.359315	28.201012
283.837454	12065.738483	28.206029
284.207053	12086.011910	28.211047
284.507885	12106.800929	28.216064
284.832333	12131.905694	28.221082
285.181432	12150.653429	28.226100
285.621175	12177.597690	28.231117
285.871991	12193.976185	28.236135
286.229965	12219.570302	28.241152
286.881962	12237.396761	28.246170
287.183924	12262.551928	28.251188
287.256818	12275.495035	28.256205
287.907597	12281.754858	28.261223
287.875112	12315.857583	28.266240
288.583279	12317.123339	28.271258
289.162516	12327.946295	28.276276
289.305259	12325.639691	28.281293
289.771591	12337.395978	28.286311
289.844124	12353.124978	28.291328
290.326304	12359.561587	28.296346
290.361992	12368.652902	28.301364
290.674602	12376.245708	28.306381
290.840664	12395.324133	28.311399
290.894443	12422.055252	28.316416
291.487643	12428.509000	28.321434
291.474745	12446.992298	28.326452
291.514040	12466.434459	28.331469
291.949629	12489.154757	28.336487
291.801743	12501.605094	28.341504
292.285568	12536.710204	28.346522
292.814882	12570.793923	28.351540
292.891990	12585.504501	28.356557
293.329265	12599.125091	28.361575
293.103399	12633.391217	28.366592
293.752854	12650.637126	28.371610
293.826065	12678.283300	28.376628
293.972048	12713.888956	28.381645
294.845264	12722.812954	28.386663
294.993311	12752.898680	28.391680
295.225372	12773.112972	28.396698
295.620499	12789.416233	28.401716
295.720308	12818.778924	28.406733
296.086261	12843.819641	28.411751
296.309589	12868.321431	28.416768
296.889673	12884.933010	28.421786
297.361082	12910.277855	28.426804
297.457768	12929.038259	28.431821
298.202040	12944.519771	28.436839
298.321014	12959.387649	28.441856
298.209951	12972.752486	28.446874
298.811496	12999.035586	28.451892
298.526209	13029.061056	28.456909
299.184157	13050.089319	28.461927
299.496540	13070.673616	28.466944
299.288822	13092.607605	28.471962
299.809908	13120.182117	28.476980
300.437647	13132.986975	28.481997
300.649108	13144.964019	28.487015
300.798814	13172.863125	28.492032
301.030202	13197.146629	28.497050
301.443653	13212.227663	28.502068
301.666889	13236.562997	28.507085
302.117388	13260.698520	28.512103
302.377751	13271.758370	28.517120
302.700871	13296.215958	28.522138
303.120119	13321.532248	28.527156
303.239111	13343.568601	28.532173
303.437426	13369.558073	28.537191
303.720782	13394.991474	28.542208
304.207574	13408.722751	28.547226
304.744155	13431.856303	28.552244
304.758716	13453.790300	28.557261
305.085897	13471.941250	28.562279
305.290167	13499.935906	28.567296
305.613709	13522.644657	28.572314
306.192631	13545.700466	28.577332
306.222819	13565.366061	28.582349
306.779082	13592.560533	28.587367
306.938997	13615.066381	28.592384
307.007407	13638.813342	28.597402
307.875070	13671.912984	28.602420
307.773640	13699.274595	28.607437
307.939748	13712.398852	28.612455
308.445408	13749.806806	28.617472
308.922236	13766.672724	28.622490
309.266628	13779.690368	28.627508
309.457418	13809.104432	28.632525
310.202802	13827.139416	28.637543
310.186302	13849.641643	28.642560
310.479498	13871.369440	28.647578
310.757326	13894.973447	28.652596
310.998123	13923.397725	28.657613
311.767429	13946.099611	28.662631
311.909164	13962.924969	28.667648
312.106835	13980.481739	28.672666
312.711801	14003.097396	28.677684
312.592479	14016.021650	28.682701
313.012894	14045.841014	28.687719
312.853293	14068.983335	28.692736
313.447117	14097.461480	28.697754
313.692458	14122.842422	28.702772
314.117199	14152.662845	28.707789
314.841723	14173.254521	28.712807
315.132884	14193.126745	28.717824
315.176202	14214.792278	28.722842
315.882130	14242.475266	28.727860
315.824802	14265.963416	28.732877
315.860906	14278.586426	28.737895
316.308538	14318.312325	28.742912
316.350636	14336.873788	28.747930
316.812156	14350.126254	28.752948
317.353757	14392.241568	28.757965
318.081895	14409.616615	28.762983
318.452423	14423.807630	28.768000
318.361754	14460.261486	28.773018
318.889964	14478.413446	28.778036
318.932486	14508.158990	28.783053
319.267606	14521.355260	28.788071
320.078798	14534.022191	28.793088
320.602053	14554.735853	28.798106
320.782031	14558.051820	28.803124
321.066923	14576.412706	28.808141
321.439064	14596.639226	28.813159
321.512570	14615.072899	28.818176
321.876754	14626.264657	28.823194
322.215825	14634.124422	28.828212
322.161247	14654.880093	28.833229
322.568372	14673.397395	28.838247
322.480292	14691.703413	28.843264
322.771904	14724.495372	28.848282
323.117480	14740.238313	28.853300
323.668417	14776.868967	28.858317
324.027572	14810.389038	28.863335
324.180637	14831.636981	28.868352
324.136477	14859.137639	28.873370
324.499595	14877.706570	28.878388
324.823676	14915.955651	28.883405
325.091830	14952.658632	28.888423
325.714868	14968.579737	28.893440
325.886684	14997.532615	28.898458
326.602276	15031.098265	28.903476
326.725300	15068.145395	28.908493
327.095776	15079.889577	28.913511
327.666628	15104.743922	28.918528
327.698277	15134.987248	28.923546
327.935508	15163.742078	28.928564
327.703731	15194.914710	28.933581
328.054650	15234.056813	28.938599
328.865799	15269.704750	28.943616
329.352544	15308.548802	28.948634
330.071438	15325.470910	28.953652
330.245186	15372.276528	28.958669
330.403131	15385.980285	28.963687
330.821959	15410.127392	28.968704
331.297400	15452.525869	28.973722
331.786876	15470.943797	28.978740
331.865958	15490.684014	28.983757
332.048079	15526.724833	28.988775
332.525885	15556.438201	28.993792
333.169526	15578.417699	28.998810
333.654209	15592.122811	29.003828
333.919416	15633.473794	29.008845
334.058048	15652.476265	29.013863
334.654622	15667.157401	29.018880
334.596660	15698.789257	29.023898
335.112570	15719.359050	29.028916
335.626448	15751.798005	29.033933
335.728262	15772.574963	29.038951
335.742740	15788.729793	29.043968
336.020776	15830.463697	29.048986
336.417873	15857.836402	29.054004
336.804139	15889.314861	29.059021
337.521078	15907.011718	29.064039
337.870003	15940.420752	29.069056
337.970357	15971.562057	29.074074
338.229053	15994.184107	29.079092
338.648473	16022.738565	29.084109
338.863444	16047.372609	29.089127
339.312234	16076.494405	29.094144
339.625251	16109.503101	29.099162
340.324545	16132.857906	29.104180
340.007211	16166.593384	29.109197
340.440766	16209.055905	29.114215
340.762992	16228.753693	29.119232
341.134607	16262.952384	29.124250
341.475200	16274.798504	29.129268
341.745762	16310.293735	29.134285
342.351120	16346.868490	29.139303
342.810523	16374.786537	29.144320
342.882645	16397.091659	29.149338
343.574135	16417.590773	29.154356
343.913989	16446.545249	29.159373
344.204202	16456.907295	29.164391
344.807585	16478.429720	29.169408
344.626186	16509.147349	29.174426
345.065753	16528.616496	29.179444
345.663782	16549.946043	29.184461
346.004123	16582.484662	29.189479
346.664766	16588.694112	29.194496
346.224628	16616.866774	29.199514
346.902302	16645.696446	29.204532
347.494211	16664.481786	29.209549
347.519481	16698.168061	29.214567
347.786220	16721.413917	29.219584
348.196820	16746.111259	29.224602
348.590921	16773.753926	29.229620
348.903193	16796.092417	29.234637
349.060533	16833.115805	29.239655
349.755739	16847.704483	29.244672
349.554029	16887.455644	29.249690
350.016710	16915.233797	29.254708
350.280559	16952.452633	29.259725
350.430744	16983.218815	29.264743
351.228422	17015.796221	29.269760
351.255074	17065.129114	29.274778
351.374075	17085.132596	29.279796
352.175045	17120.560869	29.284813
352.094344	17157.551810	29.289831
352.646146	17194.944283	29.294848
353.217563	17234.741935	29.299866
353.734701	17266.007554	29.304884
354.286386	17291.278189	29.309901
354.083016	17329.062088	29.314919
354.770974	17361.059370	29.319936
354.760525	17392.930940	29.324954
355.237810	17418.103731	29.329972
356.301884	17459.421912	29.334989
356.184870	17490.699726	29.340007
357.010087	17508.285863	29.345024
356.920575	17545.518706	29.350042
357.368306	17573.447026	29.355060
357.754186	17604.630945	29.360077
357.825084	17643.984255	29.365095
358.786899	17663.024868	29.370112
358.969200	17695.646965	29.375130
359.335882	17722.841818	29.380148
359.766131	17752.015360	29.385165
360.088872	17789.850528	29.390183
360.464920	17819.000043	29.395200
360.382111	17852.150135	29.400218
361.002937	17888.090562	29.405236
361.602738	17914.336178	29.410253
361.746082	17948.612339	29.415271
362.385962	17963.682438	29.420288
362.469667	17998.658933	29.425306
363.052869	18016.659158	29.430324
363.278060	18048.715312	29.435341
363.706924	18084.798216	29.440359
363.994720	18107.667412	29.445376
364.057601	18144.950512	29.450394
364.548328	18182.722578	29.455412
365.196017	18207.873155	29.460429
365.315762	18240.032216	29.465447
365.898232	18262.353281	29.470464
365.914547	18300.186649	29.475482
366.088574	18329.375167	29.480500
366.669258	18363.997645	29.485517
367.209708	18394.372555	29.490535
367.967415	18409.480343	29.495552
368.026356	18446.980721	29.500570
368.224757	18474.887130	29.505588
368.668876	18491.553697	29.510605
369.120330	18520.922127	29.515623
369.461952	18544.725639	29.520640
369.575182	18561.667615	29.525658
370.259658	18583.058032	29.530676
370.488319	18612.589532	29.535693
370.732013	18657.225575	29.540711
371.393189	18671.569298	29.545728
371.439015	18700.174360	29.550746
371.908518	18741.368574	29.555764
372.330269	18755.977330	29.560781
372.164982	18796.127436	29.565799
373.074873	18819.965147	29.570816
373.812184	18842.042315	29.575834
374.125016	18875.756460	29.580852
374.739312	18900.893119	29.585869
374.641666	18935.416054	29.590887
375.168607	18960.724864	29.595904
375.511670	18992.914701	29.600922
375.942195	19030.047634	29.605940
375.949448	19050.606325	29.610957
376.524295	19087.412895	29.615975
376.806484	19117.853866	29.620992
377.298499	19147.500446	29.626010
377.942265	19171.961137	29.631028
378.528191	19179.364588	29.636045
378.849965	19225.918681	29.641063
379.003786	19250.741012	29.646080
379.537288	19271.566140	29.651098
379.506420	19305.287494	29.656116
380.241697	19333.048335	29.661133
380.288706	19367.537236	29.666151
380.621002	19399.274078	29.671168
381.207998	19438.957821	29.676186
381.205508	19454.458554	29.681204
381.748881	19491.668460	29.686221
382.197359	19546.702204	29.691239
382.724854	19564.177361	29.696256
382.966758	19598.448535	29.701274
383.324396	19638.471729	29.706292
383.504516	19671.247832	29.711309
383.951225	19709.148879	29.716327
384.710216	19733.780531	29.721344
385.816999	19752.085523	29.726362
385.909567	19788.681690	29.731380
386.395038	19803.829426	29.736397
386.579865	19835.233624	29.741415
386.702056	19860.996886	29.746432
387.070883	19881.362881	29.751450
387.440401	19911.712062	29.756468
387.686935	19949.689288	29.761485
388.146857	19991.406822	29.766503
388.124937	20008.853403	29.771520
388.259346	20061.662836	29.776538
388.831507	20096.373894	29.781556
389.282592	20127.668449	29.786573
389.295670	20172.652485	29.791591
389.570824	20218.422544	29.796608
390.507177	20262.259581	29.801626
390.430641	20298.514342	29.806644
391.046091	20337.024244	29.811661
391.292179	20380.002961	29.816679
391.988652	20423.159619	29.821696
392.377671	20463.144929	29.826714
392.630375	20494.822916	29.831732
393.197119	20536.327113	29.836749
393.497620	20572.799216	29.841767
393.455592	20590.497228	29.846784
394.157766	20634.462212	29.851802
394.510861	20684.125560	29.856820
395.066999	20709.578825	29.861837
395.275753	20756.220501	29.866855
395.658988	20783.561100	29.871872
396.792932	20818.855591	29.876890
396.891643	20853.350058	29.881908
397.101957	20880.528627	29.886925
397.374935	20909.635964	29.891943
397.891496	20948.709078	29.896960
398.475725	20983.251305	29.901978
398.730360	21022.090397	29.906996
399.489574	21061.836268	29.912013
399.378909	21092.727258	29.917031
399.695774	21138.153999	29.922048
400.762834	21159.410448	29.927066
401.207103	21190.053873	29.932084
401.832266	21231.815002	29.937101
402.382202	21255.192279	29.942119
402.629091	21279.720060	29.947136
402.929893	21304.891650	29.952154
403.332630	21328.610227	29.957172
403.858928	21369.106317	29.962189
403.749312	21408.955547	29.967207
404.160422	21437.096641	29.972224
404.504390	21464.974557	29.977242
404.780881	21509.880836	29.982260
404.960131	21544.495852	29.987277
405.529748	21582.352474	29.992295
405.968517	21618.312133	29.997312
406.330233	21668.864578	30.002330
406.693874	21713.143725	30.007348
407.187584	21749.476118	30.012365
407.187817	21798.261429	30.017383
407.595436	21851.529573	30.022400
408.332093	21887.626638	30.027418
408.707215	21934.023389	30.032436
408.997763	21989.937894	30.037453
409.485000	22029.213871	30.042471
409.892705	22074.368005	30.047488
410.626210	22107.904100	30.052506
410.428598	22150.139247	30.057524
411.192916	22191.348466	30.062541
411.659079	22230.431319	30.067559
411.992462	22285.723278	30.072576
412.402387	22314.573940	30.077594
413.047397	22374.773172	30.082612
413.430593	22409.433534	30.087629
413.584245	22447.835386	30.092647
414.245679	22493.390187	30.097664
414.967445	22535.789755	30.102682
414.919543	22578.210937	30.107700
415.506301	22621.646803	30.112717
416.542124	22660.493079	30.117735
417.152290	22695.651022	30.122752
417.650917	22718.029759	30.127770
417.864551	22756.048738	30.132788
417.921573	22777.149308	30.137805
418.560198	22814.283081	30.142823
418.876000	22860.422577	30.147840
418.998828	22890.537262	30.152858
419.017023	22936.893255	30.157876
419.681692	22966.869693	30.162893
419.763060	23005.923310	30.167911
419.955953	23052.829405	30.172928
420.772744	23090.869331	30.177946
420.875109	23139.359425	30.182964
421.438404	23174.891903	30.187981
421.761238	23212.305764	30.192999
422.245414	23256.920664	30.198016
422.974094	23285.862239	30.203034
423.205194	23344.914516	30.208052
423.444125	23376.754733	30.213069
424.058952	23411.448268	30.218087
424.720323	23470.436215	30.223104
425.305867	23494.982237	30.228122
425.533590	23534.375546	30.233140
425.994450	23584.436459	30.238157
426.164478	23614.675507	30.243175
426.661877	23662.939443	30.248192
427.390049	23704.513104	30.253210
427.687350	23736.181951	30.258228
428.113387	23783.373216	30.263245
428.512786	23821.360751	30.268263
428.640428	23866.739390	30.273280
429.223589	23914.264566	30.278298
429.959522	23953.051413	30.283316
430.047456	23992.560332	30.288333
430.548982	24028.514770	30.293351
430.895640	24082.145343	30.298368
431.411147	24117.865874	30.303386
431.959532	24170.769619	30.308404
432.278129	24206.801958	30.313421
432.890784	24262.585633	30.318439
433.529480	24290.750667	30.323456
434.276899	24326.393910	30.328474
434.883092	24375.671559	30.333492
435.131161	24407.285143	30.338509
435.453431	24442.879023	30.343527
435.744349	24487.120696	30.348544
436.046202	24531.105232	30.353562
436.704627	24558.018608	30.358580
437.109223	24603.355044	30.363597
437.830819	24647.450304	30.368615
437.827337	24681.406551	30.373632
438.381409	24719.651227	30.378650
438.732414	24767.043690	30.383668
438.967312	24808.389329	30.388685
439.365895	24855.969710	30.393703
439.759684	24906.499738	30.398720
440.004927	24930.254131	30.403738
440.419869	24994.468071	30.408756
440.788932	25042.329801	30.413773
441.791673	25086.773978	30.418791
441.881429	25139.524699	30.423808
442.575670	25167.694629	30.428826
442.912822	25219.780287	30.433844
443.372745	25262.065949	30.438861
444.165405	25307.906263	30.443879
444.563128	25354.253471	30.448896
444.902922	25399.143853	30.453914
445.175556	25436.417951	30.458932
445.723304	25489.721710	30.463949
446.199609	25529.586348	30.468967
446.339982	25580.166542	30.473984
446.942631	25620.653906	30.479002
447.423342	25681.511763	30.484020
447.986802	25718.377320	30.489037
448.863149	25755.468813	30.494055
449.033136	25802.441476	30.499072
449.807137	25839.337171	30.504090
450.268269	25872.465263	30.509108
450.339831	25919.531776	30.514125
451.154085	25928.389161	30.519143
451.499948	25981.377721	30.524160
451.719392	26000.435383	30.529178
452.379748	26039.551718	30.534196
452.637376	26072.076719	30.539213
453.033265	26107.322869	30.544231
453.567925	26152.834332	30.549248
453.953778	26178.182056	30.554266
454.287890	26232.034362	30.559284
454.531275	26267.435345	30.564301
455.167668	26302.579090	30.569319
455.216098	26362.947795	30.574336
455.742191	26393.624983	30.579354
456.414939	26448.213683	30.584372
456.699797	26492.105154	30.589389
457.081838	26530.918492	30.594407
457.501845	26587.050693	30.599424
458.213337	26626.604642	30.604442
458.909370	26667.359771	30.609460
459.042330	26717.837314	30.614477
459.872825	26759.724834	30.619495
460.292546	26805.906755	30.624512
460.278004	26859.503217	30.629530
460.877649	26899.984646	30.634548
461.389128	26954.592135	30.639565
461.414162	26999.880929	30.644583
461.901639	27057.754051	30.649600
462.173432	27095.549175	30.654618
462.906574	27160.705927	30.659636
463.182652	27220.156884	30.664653
463.872927	27265.352262	30.669671
464.737585	27334.039519	30.674688
465.062987	27380.654915	30.679706
465.874721	27425.748644	30.684724
465.664256	27486.731812	30.689741
466.483424	27527.922849	30.694759
466.662119	27587.482633	30.699776
467.193008	27639.098902	30.704794
467.848391	27693.845834	30.709812
468.045448	27732.462183	30.714829
468.862901	27799.301252	30.719847
469.252155	27845.144030	30.724864
470.088454	27893.193619	30.729882
470.375475	27941.523328	30.734900
470.882503	28000.364752	30.739917
471.268625	28039.925234	30.744935
471.549537	28097.034780	30.749952
472.201285	28152.679592	30.754970
472.789375	28198.102484	30.759988
473.224614	28261.290691	30.765005
473.406602	28309.156166	30.770023
473.906363	28359.511689	30.775040
474.540425	28415.418926	30.780058
475.460277	28461.986368	30.785076
475.783309	28504.390958	30.790093
476.577923	28543.200619	30.795111
477.045206	28587.281797	30.800128
477.397784	28635.306107	30.805146
478.046596	28684.079682	30.810164
478.583480	28724.913293	30.815181
478.899220	28769.900050	30.820199
479.054185	28812.178589	30.825216
479.139114	28864.768045	30.830234
480.239016	28912.392090	30.835252
480.033191	28970.799383	30.840269
480.727848	29007.547809	30.845287
481.104594	29073.187046	30.850304
481.227883	29121.398837	30.855322
482.211409	29155.040010	30.860340
482.654973	29216.211452	30.865357
482.950644	29263.628620	30.870375
483.400844	29313.149695	30.875392
483.785527	29371.732085	30.880410
484.514724	29409.273757	30.885428
484.920216	29470.720521	30.890445
485.262859	29523.748896	30.895463
485.701755	29569.774163	30.900480
485.991514	29618.802107	30.905498
486.636891	29670.755688	30.910516
486.611288	29740.956041	30.915533
487.195178	29790.907503	30.920551
487.559672	29868.258524	30.925568
488.260954	29928.607559	30.930586
488.800983	29990.961401	30.935604
489.691570	30033.052000	30.940621
490.500261	30090.626690	30.945639
491.496625	30135.293198	30.950656
492.151283	30177.218064	30.955674
493.046873	30223.910977	30.960692
492.734129	30274.106571	30.965709
493.273688	30311.763541	30.970727
493.574612	30367.889834	30.975744
494.182543	30412.006045	30.980762
495.195599	30453.011138	30.985780
495.243180	30513.899222	30.990797
496.054771	30547.129835	30.995815
496.196448	30600.292481	31.000832
496.484674	30643.995184	31.005850
496.902614	30698.948570	31.010868
497.219728	30757.587796	31.015885
497.721700	30811.268897	31.020903
498.027435	30873.396439	31.025920
498.648479	30934.620319	31.030938
499.273731	30987.874628	31.035956
499.761968	31060.137537	31.040973
500.395261	31109.532523	31.045991
501.144155	31173.972997	31.051008
501.299894	31230.312178	31.056026
502.073591	31260.859309	31.061044
502.317250	31335.952664	31.066061
502.885933	31383.440924	31.071079
503.997974	31428.918226	31.076096
504.162735	31490.150010	31.081114
504.644666	31526.560308	31.086132
505.412594	31582.988800	31.091149
506.130768	31630.664419	31.096167
506.337269	31687.204910	31.101184
506.991142	31736.651901	31.106202
507.509994	31788.001695	31.111220
507.741754	31841.787379	31.116237
508.259521	31874.147798	31.121255
509.317426	31925.721302	31.126272
509.578294	31979.079829	31.131290
510.225671	32022.392219	31.136308
510.394950	32085.108187	31.141325
510.539189	32135.053788	31.146343
511.234339	32186.615411	31.151360
511.341345	32240.504952	31.156378
512.206925	32289.801797	31.161396
512.265987	32363.223148	31.166413
512.749743	32412.264742	31.171431
513.633959	32470.929610	31.176448
514.210892	32538.135811	31.181466
514.594515	32582.288232	31.186484
515.006580	32651.336286	31.191501
515.341984	32703.280667	31.196519
516.042610	32754.417108	31.201536
516.414568	32817.531306	31.206554
516.987186	32866.654142	31.211572
517.556559	32916.856720	31.216589
517.694468	32973.526258	31.221607
518.701694	33021.031701	31.226624
518.972841	33093.076949	31.231642
519.539063	33140.387363	31.236660
519.682120	33201.417284	31.241677
519.823102	33259.191559	31.246695
520.873891	33318.784619	31.251712
521.106518	33399.287219	31.256730
522.088641	33448.385055	31.261748
522.178265	33509.428020	31.266765
522.409925	33577.960476	31.271783
523.115806	33650.939572	31.276800
523.662279	33712.037144	31.281818
524.528289	33787.022374	31.286836
525.184730	33849.654678	31.291853
526.441521	33900.831947	31.296871
526.956993	33949.563350	31.301888
527.613548	34009.157593	31.306906
528.091684	34061.987983	31.311924
528.809889	34109.133895	31.316941
529.251099	34150.563940	31.321959
529.816637	34206.807079	31.326976
529.991718	34263.490384	31.331994
530.891124	34304.087808	31.337012
530.895100	34362.916977	31.342029
531.220470	34417.319817	31.347047
532.011676	34487.154915	31.352064
532.497820	34551.231468	31.357082
532.980558	34612.153342	31.362100
533.605742	34679.318688	31.367117
533.629346	34732.570097	31.372135
534.020708	34781.870186	31.377152
534.746959	34848.227446	31.382170
535.383962	34914.776404	31.387188
535.915830	34984.949756	31.392205
536.250258	35054.764709	31.397223
537.229790	35112.731534	31.402240
537.389029	35187.192528	31.407258
538.163054	35253.827411	31.412276
538.595997	35316.463937	31.417293
539.336254	35390.432207	31.422311
540.016310	35440.418537	31.427328
540.045252	35511.185084	31.432346
540.622499	35572.148277	31.437364
541.546084	35638.923990	31.442381
542.239959	35709.108147	31.447399
542.832644	35770.372411	31.452416
543.194343	35834.893840	31.457434
543.574554	35894.726229	31.462452
544.586977	35953.009082	31.467469
545.336114	36018.527499	31.472487
545.758334	36065.919985	31.477504
545.960925	36127.994659	31.482522
546.996308	36187.514691	31.487540
547.117478	36248.312528	31.492557
547.926055	36312.752402	31.497575
548.394906	36376.548037	31.502592
548.776933	36427.410014	31.507610
549.144316	36496.941135	31.512628
549.723696	36561.924691	31.517645
549.939804	36632.169289	31.522663
550.424222	36707.270868	31.527680
550.797800	36779.263616	31.532698
551.126433	36845.110135	31.537716
551.609893	36904.067288	31.542733
552.416110	36985.561183	31.547751
553.314269	37050.004691	31.552768
553.585236	37116.505532	31.557786
553.468702	37185.920423	31.562804
554.653542	37255.887530	31.567821
554.734852	37327.167007	31.572839
555.708581	37382.740474	31.577856
556.131939	37460.297998	31.582874
556.655882	37523.069224	31.587892
557.690261	37589.818129	31.592909
558.036916	37669.027182	31.597927
558.930347	37729.162795	31.602944
558.981153	37801.698970	31.607962
559.899528	37868.534346	31.612980
560.406350	37933.102462	31.617997
561.242072	38003.085953	31.623015
561.908680	38075.515207	31.628032
562.477248	38142.232633	31.633050
562.818986	38206.027343	31.638068
563.464035	38273.206036	31.643085
563.763048	38342.850259	31.648103
564.533507	38404.207762	31.653120
564.838469	38483.405179	31.658138
565.355794	38552.887905	31.663156
566.002931	38631.483438	31.668173
566.390503	38713.218407	31.673191
566.922189	38774.553480	31.678208
567.600512	38852.955450	31.683226
568.165593	38923.069265	31.688244
569.145168	39001.917651	31.693261
569.307435	39071.053852	31.698279
570.477100	39139.550490	31.703296
570.675015	39221.568419	31.708314
571.327358	39298.710939	31.713332
571.923236	39366.993888	31.718349
572.513155	39438.705840	31.723367
573.374581	39511.452697	31.728384
573.611629	39589.397311	31.733402
574.374758	39654.254332	31.738420
575.153624	39732.561429	31.743437
575.325002	39789.824597	31.748455
576.109644	39869.630611	31.753472
576.785059	39940.017359	31.758490
577.168451	40016.127851	31.763508
577.931937	40086.712099	31.768525
578.349992	40157.678788	31.773543
579.106244	40226.910660	31.778560
579.762000	40300.218611	31.783578
580.398725	40375.477549	31.788596
581.214824	40441.910024	31.793613
581.192844	40515.921043	31.798631
581.665162	40585.826160	31.803648
582.320580	40658.381197	31.808666
582.681977	40738.393491	31.813684
583.794283	40812.647657	31.818701
584.173759	40885.757378	31.823719
584.615785	40958.522462	31.828736
585.200453	41040.026983	31.833754
585.455758	41123.470762	31.838772
586.559561	41195.114213	31.843789
587.139646	41275.092733	31.848807
587.796663	41349.743096	31.853824
588.760024	41421.499016	31.858842
588.942740	41492.980095	31.863860
589.309214	41556.040633	31.868877
589.995581	41626.248977	31.873895
590.905260	41698.055882	31.878912
591.558746	41750.873520	31.883930
591.938824	41817.979623	31.888948
592.956649	41881.678690	31.893965
593.256515	41950.765175	31.898983
593.589303	42018.305982	31.904000
594.153685	42085.625693	31.909018
594.187742	42148.841026	31.914036
595.068764	42222.491964	31.919053
595.389932	42307.325544	31.924071
595.808747	42379.778097	31.929088
596.506566	42463.729414	31.934106
596.754158	42559.211701	31.939124
597.473672	42626.144726	31.944141
598.142807	42730.040780	31.949159
598.512732	42817.359434	31.954176
599.484618	42888.946043	31.959194
599.910012	42983.299394	31.964212
600.755268	43062.692578	31.969229
601.400648	43132.177865	31.974247
602.133034	43213.093047	31.979264
602.951109	43297.034605	31.984282
603.492972	43378.840679	31.989300
603.974879	43449.370708	31.994317
604.545008	43552.059656	31.999335
605.142373	43620.528672	32.004352
606.011510	43707.320776	32.009370
606.158438	43791.605886	32.014388
606.823837	43876.572919	32.019405
607.373907	43965.493129	32.024423
607.834919	44063.060017	32.029440
608.596404	44148.915360	32.034458
608.943095	44237.065392	32.039476
610.352234	44310.214366	32.044493
611.543062	44388.091236	32.049511
612.040055	44455.013953	32.054528
612.880297	44518.735658	32.059546
613.421596	44606.893188	32.064564
614.234186	44670.743112	32.069581
614.721702	44748.996543	32.074599
615.063619	44830.955694	32.079616
615.681975	44905.620489	32.084634
615.897786	44984.481773	32.089652
617.051227	45053.599871	32.094669
617.348068	45138.712468	32.099687
617.748359	45216.117165	32.104704
618.309735	45302.857036	32.109722
618.705497	45391.768493	32.114740
619.622191	45457.526737	32.119757
619.956351	45560.221527	32.124775
620.789208	45640.161365	32.129792
621.139408	45726.562349	32.134810
621.322564	45821.617361	32.139828
622.164328	45904.881610	32.144845
622.875745	45992.430298	32.149863
623.439175	46090.814959	32.154880
624.380403	46169.390924	32.159898
625.254892	46255.764591	32.164916
626.004015	46346.876662	32.169933
626.597088	46432.542979	32.174951
627.270762	46502.869746	32.179968
627.884218	46586.635726	32.184986
628.465828	46694.325812	32.190004
629.191002	46757.553157	32.195021
629.659314	46846.727919	32.200039
630.479506	46925.285988	32.205056
631.438608	46997.016799	32.210074
631.795190	47077.309814	32.215092
632.777933	47151.973899	32.220109
633.174084	47213.302539	32.225127
633.628786	47296.864233	32.230144
634.362731	47360.606852	32.235162
634.411848	47451.460959	32.240180
635.069193	47525.447681	32.245197
635.973361	47602.327440	32.250215
636.269924	47682.481371	32.255232
636.934542	47763.711640	32.260250
637.497746	47842.350706	32.265268
637.944745	47916.310544	32.270285
638.694518	48018.220657	32.275303
639.015997	48105.300428	32.280320
639.682979	48198.017063	32.285338
640.190640	48299.188695	32.290356
641.104112	48376.426898	32.295373
642.058737	48464.006897	32.300391
642.608713	48549.427833	32.305408
643.556354	48626.790887	32.310426
644.067455	48728.854763	32.315444
644.921934	48808.416048	32.320461
645.535615	48898.997534	32.325479
646.048933	48995.150841	32.330496
646.631412	49071.214940	32.335514
647.205962	49167.782172	32.340532
647.592809	49256.555410	32.345549
648.481016	49344.763086	32.350567
648.709502	49450.133400	32.355584
649.425989	49552.445676	32.360602
650.139043	49653.401107	32.365620
650.542651	49747.372008	32.370637
651.948941	49847.503413	32.375655
652.303173	49925.992968	32.380672
653.209294	50021.843406	32.385690
653.793108	50117.062241	32.390708
654.676125	50208.385520	32.395725
655.272302	50297.050069	32.400743
655.713511	50388.832470	32.405760
656.721263	50479.476386	32.410778
657.319099	50585.013025	32.415796
657.982404	50671.738560	32.420813
658.657451	50755.086399	32.425831
659.223674	50854.575415	32.430848
660.044594	50936.595597	32.435866
660.612503	51030.975184	32.440884
661.503223	51119.654899	32.445901
662.223179	51213.122791	32.450919
662.385711	51307.817033	32.455936
663.207928	51382.293676	32.460954
663.763244	51487.766495	32.465972
664.371799	51580.790293	32.470989
664.950042	51674.110117	32.476007
665.792539	51772.964480	32.481024
666.395518	51868.204622	32.486042
667.073671	51972.525937	32.491060
668.035566	52060.386514	32.496077
668.484803	52147.109833	32.501095
668.874872	52243.741968	32.506112
669.905565	52337.549328	32.511130
670.606344	52435.315540	32.516148
671.345396	52546.354354	32.521165
672.180368	52623.196257	32.526183
672.683596	52719.410945	32.531200
673.392307	52805.339468	32.536218
674.414650	52880.938562	32.541236
675.233876	52963.728862	32.546253
676.260995	53053.086668	32.551271
676.561041	53142.027995	32.556288
677.454506	53216.120908	32.561306
677.711171	53296.491263	32.566324
678.482348	53379.727166	32.571341
679.026488	53460.107577	32.576359
679.593641	53543.573714	32.581376
679.897885	53605.187537	32.586394
680.472875	53712.817142	32.591412
681.037236	53801.964214	32.596429
681.687573	53885.437031	32.601447
682.266513	53992.056728	32.606464
683.226238	54089.756919	32.611482
683.370948	54178.829715	32.616500
684.195628	54276.009828	32.621517
685.074945	54366.162507	32.626535
685.405507	54469.111057	32.631552
686.032282	54580.306378	32.636570
687.225473	54674.224538	32.641588
688.082673	54752.271553	32.646605
689.063567	54842.295934	32.651623
689.443129	54949.648739	32.656640
689.976991	55035.893962	32.661658
690.729936	55137.241032	32.666676
691.158844	55247.348234	32.671693
691.982196	55339.719595	32.676711
692.363541	55462.320132	32.681728
693.203010	55552.383765	32.686746
694.204411	55654.627543	32.691764
694.718539	55754.943173	32.696781
695.316282	55854.133516	32.701799
696.046840	55977.431449	32.706816
696.551497	56085.060431	32.711834
697.416960	56190.387447	32.716852
697.871935	56311.319417	32.721869
699.002192	56419.213369	32.726887
699.601927	56524.541825	32.731904
700.003050	56633.385061	32.736922
700.911665	56749.436522	32.741940
701.399629	56858.361431	32.746957
701.925623	56967.324888	32.751975
702.607902	57090.309181	32.756992
703.593435	57192.026476	32.762010
704.434672	57313.140887	32.767028
704.466038	57432.083485	32.772045
705.473085	57537.899787	32.777063
706.249009	57667.336178	32.782080
706.725902	57780.090788	32.787098
707.629805	57891.492811	32.792116
708.390535	58024.908543	32.797133
709.152299	58136.101613	32.802151
709.997305	58256.519761	32.807168
710.741440	58374.415089	32.812186
711.598597	58487.648017	32.817204
712.465294	58592.519989	32.822221
712.782197	58708.579511	32.827239
713.493730	58826.880995	32.832256
714.358511	58925.543396	32.837274
715.483001	59041.401976	32.842292
715.996142	59153.261047	32.847309
717.353642	59236.924074	32.852327
718.375157	59352.826740	32.857344
719.231583	59443.366551	32.862362
720.091848	59537.868329	32.867380
719.953541	59636.156426	32.872397
721.280160	59739.751474	32.877415
721.988061	59845.837960	32.882432
722.675191	59940.793627	32.887450
723.602232	60022.729992	32.892468
724.349423	60117.518590	32.897485
725.013197	60212.157104	32.902503
725.561670	60303.212972	32.907520
726.070510	60394.572817	32.912538
726.600358	60485.341885	32.917556
727.171037	60574.638469	32.922573
727.770723	60672.689682	32.927591
728.424538	60786.285155	32.932608
728.992610	60881.144844	32.937626
729.304236	60975.946212	32.942644
730.327154	61103.942083	32.947661
730.729581	61203.899104	32.952679
731.697132	61304.306801	32.957696
731.980377	61427.061322	32.962714
732.863627	61536.508882	32.967732
733.406575	61655.044435	32.972749
733.911902	61775.318569	32.977767
734.619223	61901.279683	32.982784
735.246400	62027.090491	32.987802
736.180452	62158.754379	32.992820
736.585675	62284.458070	32.997837
737.527793	62416.571027	33.002855
738.066903	62544.794931	33.007872
738.764917	62682.966782	33.012890
739.420716	62805.649143	33.017908
740.495098	62932.832728	33.022925
741.368292	63056.472993	33.027943
742.513748	63186.048166	33.032960
742.981240	63306.666254	33.037978
743.914296	63432.707006	33.042996
744.369233	63573.156157	33.048013
745.359210	63688.583216	33.053031
746.109798	63832.221457	33.058048
746.881186	63958.127804	33.063066
747.889143	64082.384080	33.068084
748.369667	64214.205640	33.073101
749.704162	64326.589689	33.078119
750.761173	64440.473962	33.083136
751.650965	64563.570670	33.088154
752.697508	64671.225595	33.093172
753.134866	64787.887851	33.098189
754.058496	64908.762394	33.103207
754.200071	65012.813899	33.108224
755.307035	65126.681077	33.113242
756.124585	65247.126328	33.118260
756.722879	65361.647697	33.123277
757.852748	65469.356241	33.128295
759.062773	65591.653992	33.133312
759.426792	65705.071819	33.138330
760.208670	65815.191116	33.143348
760.436166	65936.635435	33.148365
761.502190	66046.911322	33.153383
762.024692	66156.057531	33.158400
762.628774	66280.033420	33.163418
763.458164	66398.782966	33.168436
764.274610	66521.290267	33.173453
764.977477	66645.896813	33.178471
765.815086	66770.159458	33.183488
766.018222	66898.244694	33.188506
767.050346	67015.402856	33.193524
768.125980	67145.798314	33.198541
769.216478	67261.216092	33.203559
769.962919	67377.999916	33.208576
770.307310	67503.416745	33.213594
771.702615	67611.282216	33.218612
772.208803	67737.514528	33.223629
773.153599	67850.373999	33.228647
773.317672	67974.053307	33.233664
774.025198	68090.866502	33.238682
775.005633	68200.700098	33.243700
775.847147	68321.216082	33.248717
776.735403	68445.587798	33.253735
777.209614	68548.350273	33.258752
777.552446	68667.667215	33.263770
778.353908	68776.142515	33.268788
779.035686	68908.289349	33.273805
779.825189	69021.598024	33.278823
780.692203	69146.464201	33.283840
780.965980	69279.085356	33.288858
781.815052	69408.071847	33.293876
782.710639	69546.870065	33.298893
783.185782	69675.173896	33.303911
784.501526	69791.757001	33.308928
785.301408	69945.469291	33.313946
786.334033	70060.146982	33.318964
786.837119	70198.211327	33.323981
787.761951	70332.166792	33.328999
788.832802	70458.018669	33.334016
789.519787	70588.923264	33.339034
790.494241	70706.851265	33.344052
791.477212	70835.761113	33.349069
791.884125	70959.000491	33.354087
792.954367	71096.237252	33.359104
793.615853	71220.454079	33.364122
794.662442	71335.376618	33.369140
794.916979	71478.928002	33.374157
795.859800	71607.178916	33.379175
796.673555	71735.161054	33.384192
797.604894	71883.870465	33.389210
798.134251	72000.943309	33.394228
799.267950	72140.180720	33.399245
800.076567	72265.239269	33.404263
800.944907	72404.945871	33.409280
801.415307	72538.768918	33.414298
802.287132	72663.111145	33.419316
802.935587	72805.215243	33.424333
803.738480	72948.432984	33.429351
804.630920	73079.704626	33.434368
805.286922	73238.757067	33.439386
806.122466	73372.910736	33.444404
807.002833	73504.066810	33.449421
807.515725	73652.231524	33.454439
808.493232	73802.255560	33.459456
809.230928	73941.411927	33.464474
810.226300	74094.514660	33.469492
810.454040	74235.287458	33.474509
811.627687	74374.564333	33.479527
812.328245	74527.864256	33.484544
813.280537	74679.119026	33.489562
814.444178	74825.736141	33.494580
814.730797	74973.314854	33.499597
815.500610	75124.602854	33.504615
816.705679	75262.811480	33.509632
817.209223	75417.503547	33.514650
817.953273	75558.642336	33.519668
818.993301	75714.379939	33.524685
820.137065	75864.416053	33.529703
821.000012	75992.763105	33.534720
821.925686	76144.525728	33.539738
823.043682	76295.410185	33.544756
823.887784	76424.047472	33.549773
824.849893	76568.717393	33.554791
825.708639	76696.740393	33.559808
826.081206	76831.143612	33.564826
827.163296	76966.436093	33.569844
827.878469	77115.982334	33.574861
828.327024	77246.182347	33.579879
829.538561	77389.734974	33.584896
829.402978	77532.948078	33.589914
830.567987	77655.246505	33.594932
832.054602	77790.464601	33.599949
832.702388	77934.354200	33.604967
833.303091	78055.976398	33.609984
834.072667	78198.879905	33.615002
834.858481	78331.775624	33.620020
835.276584	78461.583026	33.625037
836.240408	78615.873699	33.630055
837.530418	78750.750625	33.635072
838.184643	78906.884428	33.640090
839.039081	79039.469447	33.645108
839.738513	79181.941778	33.650125
840.488386	79332.389100	33.655143
841.060114	79472.797059	33.660160
842.106884	79625.461772	33.665178
842.986796	79784.088243	33.670196
844.147448	79920.442114	33.675213
844.782183	80068.642598	33.680231
845.757283	80216.844791	33.685248
846.631991	80377.298058	33.690266
847.624708	80516.940925	33.695284
848.205634	80663.174330	33.700301
850.132943	80794.137720	33.705319
851.681203	80919.287930	33.710336
852.241451	81052.388902	33.715354
853.149712	81196.610763	33.720372
853.899691	81322.318851	33.725389
854.254467	81457.670162	33.730407
854.904883	81593.884390	33.735424
855.497951	81740.122781	33.740442
856.289332	81882.394648	33.745460
857.186531	82036.523774	33.750477
858.023816	82187.893050	33.755495
858.971305	82342.794055	33.760512
859.704393	82497.908651	33.765530
860.191630	82643.967915	33.770548
861.252070	82792.482920	33.775565
862.078860	82958.909051	33.780583
863.032965	83101.661466	33.785600
863.776068	83264.560942	33.790618
864.851548	83422.712546	33.795636
865.666471	83585.747962	33.800653
866.536187	83750.262209	33.805671
867.425341	83900.084328	33.810688
868.353079	84053.741259	33.815706
869.303982	84200.847398	33.820724
869.934173	84365.728271	33.825741
870.539712	84532.290963	33.830759
871.716523	84683.690332	33.835776
872.580012	84847.916128	33.840794
873.050355	85009.063596	33.845812
874.002047	85162.717664	33.850829
874.754764	85344.648793	33.855847
875.762388	85498.953862	33.860864
876.469365	85675.245205	33.865882
877.371840	85838.649111	33.870900
878.483545	85999.950674	33.875917
879.011038	86173.788914	33.880935
880.028515	86331.248806	33.885952
881.216022	86504.638881	33.890970
881.526473	86670.228046	33.895988
882.607663	86840.373323	33.901005
883.502955	87023.939184	33.906023
884.657261	87174.561323	33.911040
885.497372	87349.957561	33.916058
886.128302	87522.972560	33.921076
887.167055	87689.802789	33.926093
887.973188	87858.817661	33.931111
889.275416	88002.321187	33.936128
890.187614	88147.509868	33.941146
890.971457	88302.218494	33.946164
891.836916	88445.037524	33.951181
892.667604	88602.625836	33.956199
893.573296	88762.113817	33.961216
894.581168	88918.086706	33.966234
895.572674	89077.860066	33.971252
896.485869	89238.995289	33.976269
897.209961	89407.718443	33.981287
898.067584	89557.898628	33.986304
898.879670	89721.838166	33.991322
899.311279	89879.678083	33.996340
900.577723	90053.176276	34.001357
900.956163	90229.524499	34.006375
901.892207	90397.789389	34.011392
903.300683	90578.304979	34.016410
903.991878	90748.416340	34.021428
905.087973	90909.785849	34.026445
905.565228	91100.730117	34.031463
906.313716	91262.311286	34.036480
907.558113	91449.100437	34.041498
908.036272	91628.347330	34.046516
909.139941	91794.404706	34.051533
910.257896	91988.863913	34.056551
911.389319	92168.544920	34.061568
912.052744	92340.621427	34.066586
912.709684	92521.566891	34.071604
914.241507	92699.622542	34.076621
915.090097	92883.051633	34.081639
916.438942	93047.298759	34.086656
917.457970	93217.164640	34.091674
918.132336	93406.227625	34.096692
919.852850	93562.296732	34.101709
920.537085	93730.411376	34.106727
922.006050	93889.555775	34.111744
922.559491	94052.732181	34.116762
923.551821	94224.381707	34.121780
924.632824	94385.264332	34.126797
925.677126	94556.698754	34.131815
926.288914	94717.623068	34.136832
927.171604	94886.864882	34.141850
928.032250	95054.870932	34.146868
929.087739	95210.516084	34.151885
929.968998	95387.565883	34.156903
930.925024	95547.255193	34.161920
931.789811	95726.183716	34.166938
932.508892	95906.631406	34.171956
933.793547	96048.964365	34.176973
934.423697	96229.840541	34.181991
935.377986	96398.542932	34.187008
936.125524	96574.154838	34.192026
936.927909	96750.240010	34.197044
938.315101	96918.444048	34.202061
938.635809	97102.884499	34.207079
939.594778	97285.391560	34.212096
941.007726	97454.709076	34.217114
941.522461	97637.754171	34.222132
942.693119	97819.154085	34.227149
943.320348	97993.612169	34.232167
944.226787	98179.324900	34.237184
945.496689	98347.374408	34.242202
946.083530	98538.934816	34.247220
947.237591	98715.621547	34.252237
948.021389	98900.315371	34.257255
948.957474	99079.895695	34.262272
949.912333	99270.261448	34.267290
950.674018	99439.718952	34.272308
951.561321	99615.038014	34.277325
951.968033	99799.642444	34.282343
952.995992	99979.138056	34.287360
953.970575	100157.947375	34.292378
954.445372	100351.616591	34.297396
956.016162	100523.986591	34.302413
956.857789	100718.351423	34.307431
957.714684	100904.510309	34.312448
958.790038	101088.779511	34.317466
959.620283	101293.197922	34.322484
960.869594	101480.138269	34.327501
962.081778	101664.230774	34.332519
962.712055	101850.813871	34.337536
964.109096	102034.625283	34.342554
964.659599	102235.729222	34.347572
965.246961	102416.524079	34.352589
966.747883	102624.261339	34.357607
967.779749	102814.444697	34.362624
968.523872	103006.329485	34.367642
969.398418	103210.774905	34.372660
970.409677	103404.777609	34.377677
971.376282	103598.263621	34.382695
972.085593	103802.335789	34.387712
973.662316	103995.040224	34.392730
974.432411	104211.237152	34.397748
975.610884	104393.075341	34.402765
976.725440	104589.387323	34.407783
977.610412	104801.137898	34.412800
979.047011	104989.326547	34.417818
979.424009	105193.179578	34.422836
980.722444	105376.625834	34.427853
981.848183	105585.094687	34.432871
982.210759	105784.180307	34.437888
983.612355	105988.731557	34.442906
984.670483	106179.904081	34.447924
985.935379	106380.782928	34.452941
986.506819	106583.601513	34.457959
987.145246	106784.726184	34.462976
988.340169	106991.459710	34.467994
989.280821	107201.593056	34.473012
990.394206	107411.636229	34.478029
991.441858	107610.736541	34.483047
993.054952	107804.248270	34.488064
995.093135	107984.544588	34.493082
996.265967	108173.420185	34.498100
997.282937	108349.593994	34.503117
998.479854	108524.067400	34.508135
998.952537	108713.493051	34.513152
1000.206118	108894.317708	34.518170
1001.374761	109072.915753	34.523188
1001.951354	109264.418022	34.528205
1002.786645	109449.634585	34.533223
1003.708731	109629.796975	34.538240
1004.633203	109813.494055	34.543258
1005.519042	109999.010051	34.548276
1006.623637	110188.063135	34.553293
1007.468090	110383.671067	34.558311
1008.241047	110578.734891	34.563328
1009.521458	110761.797009	34.568346
1010.261250	110969.979134	34.573364
1011.238888	111167.306093	34.578381
1012.052604	111360.582792	34.583399
1012.814224	111579.925574	34.588416
1013.789565	111764.792877	34.593434
1014.953151	111985.883968	34.598452
1015.794148	112177.578557	34.603469
1016.770757	112371.228219	34.608487
1017.577966	112582.439052	34.613504
1018.757535	112764.517887	34.618522
1019.606765	112960.384238	34.623540
1020.686143	113158.684206	34.628557
1022.001648	113350.688695	34.633575
1022.803476	113540.410419	34.638592
1023.727231	113745.365645	34.643610
1024.592915	113941.945670	34.648628
1025.560135	114140.043186	34.653645
1026.113452	114354.539919	34.658663
1027.493461	114560.908056	34.663680
1028.412139	114767.024507	34.668698
1029.379198	114996.622109	34.673716
1030.238894	115202.409468	34.678733
1031.187595	115426.059343	34.683751
1032.363113	115647.266468	34.688768
1033.551854	115857.603147	34.693786
1034.514271	116078.722172	34.698804
1035.295506	116311.072432	34.703821
1036.410448	116531.827774	34.708839
1037.219697	116755.777327	34.713856
1038.474937	116984.431438	34.718874
1039.518614	117220.191974	34.723892
1040.412488	117452.697746	34.728909
1041.926765	117678.299307	34.733927
1042.659337	117905.881520	34.738944
1043.785940	118131.930782	34.743962
1044.600043	118363.519594	34.748980
1045.740458	118588.569256	34.753997
1047.075048	118825.359376	34.759015
1047.664094	119076.072648	34.764032
1049.015863	119308.530634	34.769050
1050.156522	119547.550739	34.774068
1051.255520	119781.169294	34.779085
1052.453940	120003.166825	34.784103
1053.177471	120246.062843	34.789120
1054.235188	120487.930059	34.794138
1055.186429	120733.909661	34.799156
1056.340775	120981.162961	34.804173
1057.588791	121225.678552	34.809191
1058.436938	121469.945421	34.814208
1059.724949	121708.629574	34.819226
1060.658670	121963.555933	34.824244
1061.709688	122207.554713	34.829261
1063.328012	122428.272266	34.834279
1063.861607	122683.258262	34.839296
1065.468437	122917.895270	34.844314
1066.632745	123160.540011	34.849332
1067.307176	123412.695831	34.854349
1068.916046	123645.665539	34.859367
1069.885565	123876.550277	34.864384
1071.230777	124105.942784	34.869402
1072.591108	124331.228602	34.874420
1073.558857	124564.995686	34.879437
1074.710976	124803.334437	34.884455
1075.281880	125046.738862	34.889472
1076.910833	125273.254746	34.894490
1077.545116	125507.578494	34.899508
1078.681840	125740.477753	34.904525
1079.822952	125968.105949	34.909543
1080.657445	126213.288604	34.914560
1081.692361	126449.809427	34.919578
1082.893746	126685.049919	34.924596
1083.579436	126940.186547	34.929613
1085.052404	127175.930986	34.934631
1085.693125	127425.046319	34.939648
1086.536589	127676.120054	34.944666
1088.174457	127912.844227	34.949684
1089.073835	128134.052031	34.954701
1090.594479	128359.861078	34.959719
1091.292508	128592.994029	34.964736
1092.601567	128815.900871	34.969754
1093.598530	129041.104267	34.974772
1094.468962	129276.761543	34.979789
1095.682383	129504.290093	34.984807
1096.839050	129753.199697	34.989824
1097.929895	129981.753310	34.994842
1098.848241	130211.249691	34.999860
1100.106320	130447.840530	35.004877
1101.400746	130679.635876	35.009895
1102.139930	130915.530043	35.014912
1103.100302	131154.292174	35.019930
1104.554769	131396.536416	35.024948
1105.262357	131645.167636	35.029965
1106.506132	131891.557412	35.034983
1107.544253	132138.452071	35.040000
1108.352970	132389.075256	35.045018
1109.552095	132641.740217	35.050036
1110.904940	132887.359172	35.055053
1111.992365	133137.802820	35.060071
1113.141087	133398.316094	35.065088
1114.019052	133641.382551	35.070106
1115.356352	133901.868799	35.075124
1117.150225	134139.096025	35.080141
1118.826825	134380.451660	35.085159
1119.909434	134604.083397	35.090176
1120.918887	134839.809956	35.095194
1121.833696	135096.902120	35.100212
1123.458528	135334.153372	35.105229
1124.500027	135570.184214	35.110247
1125.323166	135821.275533	35.115264
1126.515364	136062.977228	35.120282
1127.574180	136298.097708	35.125300
1128.564591	136557.382156	35.130317
1129.544086	136794.192750	35.135335
1130.615335	137050.982912	35.140352
1131.477468	137314.034485	35.145370
1132.679149	137562.325537	35.150388
1133.338448	137838.346409	35.155405
1134.497101	138107.453556	35.160423
1135.701071	138360.910282	35.165440
1137.065467	138635.261950	35.170458
1138.409258	138895.723550	35.175476
1139.544008	139149.717527	35.180493
1140.691817	139411.001572	35.185511
1141.830546	139680.999540	35.190528
1142.759427	139939.876816	35.195546
1143.942942	140208.857309	35.200564
1145.184075	140472.302313	35.205581
1146.657143	140728.458538	35.210599
1147.698012	140988.922952	35.215616
1148.758695	141244.352344	35.220634
1149.923777	141521.664024	35.225652
1151.021629	141780.793733	35.230669
1152.419096	142044.618178	35.235687
1153.389059	142314.284558	35.240704
1154.393747	142580.498373	35.245722
1155.665006	142853.213152	35.250740
1156.415300	143118.763030	35.255757
1157.685091	143387.145651	35.260775
1158.735371	143659.421411	35.265792
1159.966764	143923.452475	35.270810
1161.237245	144199.271997	35.275828
1162.641087	144463.874672	35.280845
1163.940379	144743.624734	35.285863
1164.492996	145014.966069	35.290880
1165.984156	145262.732879	35.295898
1167.245495	145526.707676	35.300916
1168.498423	145792.359742	35.305933
1169.325967	146025.873736	35.310951
1170.268636	146295.879718	35.315968
1171.389807	146559.365409	35.320986
1172.480418	146808.046112	35.326004
1173.862573	147096.842990	35.331021
1174.471476	147353.494946	35.336039
1175.527647	147622.667907	35.341056
1176.553851	147900.230543	35.346074
1178.011448	148174.705797	35.351092
1179.050538	148449.962412	35.356109
1180.410130	148736.341197	35.361127
1181.876894	149025.101497	35.366144
1182.288508	149305.224009	35.371162
1183.855602	149598.956457	35.376180
1184.650269	149893.516301	35.381197
1185.898434	150175.143429	35.386215
1186.743340	150487.988142	35.391232
1187.871442	150782.309812	35.396250
1189.265279	151081.358755	35.401268
1190.150760	151391.401464	35.406285
1191.232838	151699.752804	35.411303
1192.507869	152010.091483	35.416320
1193.422651	152314.492952	35.421338
1195.061395	152627.744620	35.426356
1196.238020	152963.690041	35.431373
1197.239500	153270.685063	35.436391
1198.487239	153591.454601	35.441408
1199.621822	153907.438315	35.446426
1201.343632	154219.141989	35.451444
1202.085497	154560.297627	35.456461
1203.196035	154865.042390	35.461479
1204.786544	155188.089957	35.466496
1205.473251	155528.096316	35.471514
1207.032870	155841.831370	35.476532
1208.476337	156168.336221	35.481549
1210.094372	156499.178556	35.486567
1211.272645	156812.426243	35.491584
1212.029037	157129.576932	35.496602
1213.650517	157459.361265	35.501620
1214.937733	157782.213990	35.506637
1216.250954	158106.257474	35.511655
1217.992560	158406.117964	35.516672
1219.299657	158729.038536	35.521690
1221.108781	159019.733575	35.526708
1223.385371	159306.167294	35.531725
1224.944436	159581.355048	35.536743
1226.416947	159866.466617	35.541760
1227.537439	160149.405577	35.546778
1229.207072	160424.098760	35.551796
1230.014567	160717.254850	35.556813
1231.219939	160988.260696	35.561831
1232.637409	161258.801999	35.566848
1233.686458	161546.012357	35.571866
1234.581527	161815.882377	35.576884
1235.435591	162103.014628	35.581901
1236.519870	162391.239987	35.586919
1237.887829	162674.485393	35.591936
1238.686915	162964.639440	35.596954
1240.040176	163252.509204	35.601972
1240.992014	163544.430920	35.606989
1242.109235	163836.289310	35.612007
1243.780257	164133.006309	35.617024
1244.739907	164424.222360	35.622042
1245.749957	164710.039979	35.627060
1247.027207	165006.510915	35.632077
1248.285946	165293.357152	35.637095
1249.628376	165577.171856	35.642112
1250.730523	165860.799721	35.647130
1251.738358	166153.377209	35.652148
1252.785572	166443.399926	35.657165
1253.477787	166733.292862	35.662183
1254.790971	167031.040630	35.667200
1255.947133	167350.183126	35.672218
1257.194043	167650.458311	35.677236
1258.304034	167972.404373	35.682253
1259.486907	168284.393072	35.687271
1260.960715	168593.455676	35.692288
1261.971295	168918.724056	35.697306
1263.051293	169229.759380	35.702324
1264.007670	169556.690895	35.707341
1264.753985	169893.099966	35.712359
1266.260262	170207.865697	35.717376
1267.662330	170558.510004	35.722394
1269.342453	170879.037922	35.727412
1270.554877	171226.812896	35.732429
1272.197940	171554.800264	35.737447
1273.636548	171874.245701	35.742464
1274.736197	172220.473362	35.747482
1276.267665	172554.221942	35.752500
1277.605641	172878.195751	35.757517
1278.771975	173221.374379	35.762535
1279.901250	173551.554550	35.767552
1280.967271	173894.120185	35.772570
1282.430773	174236.914586	35.777588
1283.744466	174577.883447	35.782605
1284.873972	174930.687069	35.787623
1286.039587	175272.040685	35.792640
1286.958634	175623.044075	35.797658
1288.522870	175975.034931	35.802676
1289.398366	176337.192986	35.807693
1290.898040	176687.054984	35.812711
1292.326637	177046.690446	35.817728
1293.430098	177418.616227	35.822746
1294.730788	177767.478170	35.827764
1296.329201	178133.375616	35.832781
1297.393461	178498.513626	35.837799
1298.666353	178849.481841	35.842816
1300.212443	179221.297378	35.847834
1301.985516	179573.343040	35.852852
1303.138829	179935.418225	35.857869
1304.546989	180286.145721	35.862887
1306.240600	180657.985590	35.867904
1307.426433	181016.547524	35.872922
1308.603528	181357.979380	35.877940
1310.106490	181720.187228	35.882957
1311.753831	182066.292962	35.887975
1312.781503	182421.463924	35.892992
1314.019739	182789.954772	35.898010
1315.253150	183148.891699	35.903028
1316.239471	183512.453810	35.908045
1317.301398	183884.598757	35.913063
1319.067812	184237.705416	35.918080
1320.346248	184613.957507	35.923098
1321.844455	184983.372655	35.928116
1323.053223	185330.397180	35.933133
1324.238110	185698.066546	35.938151
1326.025399	186063.658869	35.943168
1327.047761	186426.409701	35.948186
1328.303535	186795.953330	35.953204
1329.507400	187156.127686	35.958221
1330.492489	187536.522891	35.963239
1332.463323	187905.752805	35.968256
1333.753405	188263.635270	35.973274
1335.207422	188612.594753	35.978292
1336.625475	188971.564928	35.983309
1337.658762	189312.347272	35.988327
1339.134100	189656.041739	35.993344
1340.206179	190008.233559	35.998362
1341.433485	190354.588072	36.003380
1343.146479	190712.720734	36.008397
1344.104658	191065.788273	36.013415
1345.745765	191423.213589	36.018432
1346.841793	191807.109743	36.023450
1347.978442	192154.441926	36.028468
1349.899912	192516.422929	36.033485
1351.422452	192867.567378	36.038503
1352.786915	193219.260444	36.043520
1354.283869	193586.383086	36.048538
1355.535271	193938.746411	36.053556
1357.188892	194300.820388	36.058573
1359.089885	194645.285962	36.063591
1360.286790	194997.740524	36.068608
1361.599017	195345.442812	36.073626
1362.953945	195706.152457	36.078644
1364.539563	196046.907392	36.083661
1365.884320	196406.264346	36.088679
1366.803667	196743.921097	36.093696
1368.406570	197114.449398	36.098714
1369.622705	197486.833726	36.103732
1370.500943	197840.778595	36.108749
1371.954232	198220.516795	36.113767
1373.441214	198598.893207	36.118784
1374.335889	198959.620909	36.123802
1375.421602	199340.302247	36.128820
1376.562753	199717.586815	36.133837
1377.617437	200108.155047	36.138855
1379.437004	200501.024254	36.143872
1380.608456	200901.379131	36.148890
1381.698735	201295.655588	36.153908
1383.409978	201694.008894	36.158925
1384.547829	202094.782548	36.163943
1386.063921	202496.308655	36.168960
1387.358969	202893.277420	36.173978
1388.743058	203297.559623	36.178996
1390.180937	203707.472542	36.184013
1391.268455	204111.046499	36.189031
1393.016950	204511.580683	36.194048
1394.700310	204932.252289	36.199066
1395.786851	205347.742895	36.204084
1397.769110	205745.363059	36.209101
1399.218134	206169.267331	36.214119
1400.786666	206572.838912	36.219136
1402.209602	206965.415536	36.224154
1403.279131	207380.920234	36.229172
1405.064405	207776.361601	36.234189
1406.193027	208185.385271	36.239207
1407.614057	208586.490425	36.244224
1409.605977	208988.455734	36.249242
1410.680580	209399.729417	36.254260
1412.414665	209805.626876	36.259277
1413.334794	210205.210283	36.264295
1414.737918	210609.591896	36.269312
1416.329615	211022.109095	36.274330
1417.452303	211423.264969	36.279348
1419.054737	211830.565607	36.284365
1420.238632	212250.521027	36.289383
1421.599537	212661.001962	36.294400
1423.242904	213077.457181	36.299418
1424.717494	213492.062942	36.304436
1426.002633	213895.730664	36.309453
1427.505603	214310.284854	36.314471
1428.945391	214701.486421	36.319488
1430.600889	215083.308074	36.324506
1432.119946	215478.334893	36.329524
1433.607085	215870.498839	36.334541
1434.952019	216263.856210	36.339559
1436.014966	216650.988670	36.344576
1437.647268	217038.257365	36.349594
1438.981027	217442.415471	36.354612
1440.417010	217841.402723	36.359629
1441.937185	218243.476273	36.364647
1443.273072	218647.816923	36.369664
1444.584174	219039.845355	36.374682
1445.744961	219450.364522	36.379700
1446.874930	219909.807286	36.384717
1448.692360	220331.473102	36.389735
1450.808289	220744.786157	36.394752
1452.524398	221143.588151	36.399770
1453.956860	221553.969434	36.404788
1455.590661	221966.858972	36.409805
1456.797096	222369.483359	36.414823
1457.902785	222781.294875	36.419840
1459.548254	223197.946285	36.424858
1461.014799	223615.466984	36.429876
1462.612991	224035.126467	36.434893
1463.447672	224453.491167	36.439911
1464.818673	224868.924193	36.444928
1466.529710	225298.297699	36.449946
1467.887185	225723.006838	36.454964
1469.434534	226148.067183	36.459981
1470.505354	226589.184099	36.464999
1472.307582	227023.628800	36.470016
1474.023388	227445.541778	36.475034
1475.216930	227883.239566	36.480052
1477.054102	228323.321888	36.485069
1478.184859	228759.940895	36.490087
1479.886314	229191.260171	36.495104
1481.632630	229634.537027	36.500122
1482.858687	230077.139215	36.505140
1484.370471	230500.721564	36.510157
1485.874912	230953.364691	36.515175
1487.166238	231379.195997	36.520192
1489.203613	231815.472195	36.525210
1490.498412	232252.913707	36.530228
1492.385619	232694.348336	36.535245
1493.856121	233135.192639	36.540263
1495.046318	233573.620607	36.545280
1496.619448	234011.961260	36.550298
1497.876215	234457.340695	36.555316
1499.236683	234901.967655	36.560333
1500.991771	235356.792878	36.565351
1502.048278	235802.031328	36.570368
1504.113447	236258.255783	36.575386
1505.601816	236713.103374	36.580404
1506.954741	237156.848633	36.585421
1508.170918	237608.568308	36.590439
1509.669516	238067.228006	36.595456
1511.465441	238508.287177	36.600474
1512.581984	238973.184829	36.605492
1514.132567	239428.867323	36.610509
1515.647100	239886.614406	36.615527
1517.294281	240344.543884	36.620544
1519.396333	240806.209661	36.625562
1520.883877	241257.969433	36.630580
1522.393623	241716.940735	36.635597
1524.067587	242157.189867	36.640615
1525.474659	242612.064833	36.645632
1526.801658	243051.077464	36.650650
1528.574886	243506.782873	36.655668
1530.180335	243925.886526	36.660685
1531.965628	244367.162992	36.665703
1533.196204	244794.890612	36.670720
1535.179914	245219.649585	36.675738
1536.308535	245655.879899	36.680756
1537.900089	246074.379687	36.685773
1538.950990	246511.614883	36.690791
1540.052814	246963.169475	36.695808
1541.719793	247387.602961	36.700826
1542.774736	247860.250918	36.705844
1544.240586	248300.316149	36.710861
1545.829260	248765.358120	36.715879
1547.137266	249228.592622	36.720896
1548.701111	249688.711758	36.725914
1549.908577	250173.175501	36.730932
1551.041822	250646.525582	36.735949
1552.780290	251124.374298	36.740967
1554.407010	251620.201946	36.745984
1556.043433	252096.391958	36.751002
1557.302865	252585.092172	36.756020
1559.363787	253076.861407	36.761037
1560.789641	253560.048003	36.766055
1562.863720	254051.587305	36.771072
1564.347519	254538.753435	36.776090
1565.974688	255028.893844	36.781108
1567.634969	255502.974285	36.786125
1568.896936	256014.793738	36.791143
1570.345748	256519.114105	36.796160
1572.210719	257018.564848	36.801178
1573.697370	257523.285910	36.806196
1574.977640	258014.602883	36.811213
1576.916558	258525.143246	36.816231
1578.454884	259033.031690	36.821248
1579.854953	259548.081380	36.826266
1581.493001	260069.137865	36.831284
1582.935352	260567.592334	36.836301
1584.390664	261085.071749	36.841319
1585.861375	261604.199813	36.846336
1587.918464	262125.263329	36.851354
1589.136838	262638.082049	36.856372
1590.772358	263157.868526	36.861389
1592.875794	263692.032103	36.866407
1594.214784	264208.183667	36.871424
1595.983288	264712.807263	36.876442
1597.526852	265250.085489	36.881460
1599.664069	265770.118265	36.886477
1601.416090	266278.325557	36.891495
1602.890939	266811.574969	36.896512
1604.688071	267318.300676	36.901530
1606.130711	267841.875938	36.906548
1607.777247	268359.117104	36.911565
1609.380039	268875.806117	36.916583
1610.707786	269398.382682	36.921600
1612.670173	269922.784586	36.926618
1614.279284	270438.099072	36.931636
1615.576603	270949.730130	36.936653
1617.813846	271477.844381	36.941671
1619.126596	272002.299994	36.946688
1621.327745	272507.378291	36.951706
1622.656338	273014.047777	36.956724
1624.141038	273541.165386	36.961741
1625.813102	274064.440795	36.966759
1627.443731	274584.089557	36.971776
1629.240113	275097.486401	36.976794
1630.561473	275622.417270	36.981812
1632.413010	276135.752295	36.986829
1634.553270	276653.382519	36.991847
1635.852548	277172.039535	36.996864
1637.458885	277649.416689	37.001882
1638.958907	278142.331282	37.006900
1640.463396	278643.931690	37.011917
1642.133059	279127.544349	37.016935
1643.699192	279645.110365	37.021952
1645.185854	280152.095562	37.026970
1646.536109	280652.040264	37.031988
1647.859767	281158.668862	37.037005
1649.538805	281681.621793	37.042023
1650.979229	282201.386649	37.047040
1653.133685	282723.750271	37.052058
1654.376665	283235.797290	37.057076
1656.037249	283770.305231	37.062093
1657.519579	284300.878322	37.067111
1659.196686	284824.635452	37.072128
1660.791465	285358.387301	37.077146
1662.500335	285899.713606	37.082164
1664.092484	286432.598745	37.087181
1666.132218	286965.255843	37.092199
1667.466461	287521.015483	37.097216
1669.448547	288060.739797	37.102234
1671.135284	288601.450720	37.107252
1672.687173	289155.593512	37.112269
1674.658781	289700.012655	37.117287
1675.951359	290253.330327	37.122304
1677.916947	290807.449166	37.127322
1679.599365	291355.541769	37.132340
1681.643506	291894.682340	37.137357
1683.997212	292435.700031	37.142375
1685.587247	292986.645866	37.147392
1687.135477	293537.316798	37.152410
1688.538744	294086.764617	37.157428
1690.259111	294635.395661	37.162445
1692.126564	295187.505084	37.167463
1693.501146	295747.338493	37.172480
1695.105236	296305.200997	37.177498
1696.708404	296863.746719	37.182516
1697.983264	297432.808279	37.187533
1699.942770	298011.786572	37.192551
1701.326445	298577.928789	37.197568
1702.768809	299157.189486	37.202586
1704.529560	299742.515551	37.207604
1705.850244	300333.879573	37.212621
1707.533012	300922.031080	37.217639
1709.103767	301519.036208	37.222656
1710.870879	302108.182803	37.227674
1713.040132	302706.809117	37.232692
1714.600637	303307.563986	37.237709
1716.740237	303901.057458	37.242727
1718.326446	304505.940316	37.247744
1719.823054	305097.856073	37.252762
1721.813695	305688.010316	37.257780
1723.424248	306297.905983	37.262797
1725.153540	306891.320864	37.267815
1726.749890	307503.013778	37.272832
1728.406031	308102.299135	37.277850
1730.280770	308720.185029	37.282868
1731.511049	309329.157188	37.287885
1733.444852	309942.148379	37.292903
1735.065170	310580.734706	37.297920
1737.125973	311168.782760	37.302938
1738.750086	311787.626772	37.307956
1741.081722	312389.944102	37.312973
1743.695880	312984.363234	37.317991
1745.142347	313593.673956	37.323008
1747.049432	314181.674152	37.328026
1748.928635	314765.484372	37.333044
1750.486896	315362.598702	37.338061
1752.088367	315937.811660	37.343079
1753.969629	316518.738336	37.348096
1755.888830	317080.075810	37.353114
1757.733034	317629.715025	37.358132
1759.018121	318201.280271	37.363149
1761.082076	318780.939703	37.368167
1762.579840	319360.941683	37.373184
1764.315480	319925.892679	37.378202
1766.407161	320501.165716	37.383220
1767.712697	321084.384320	37.388237
1769.393873	321660.603976	37.393255
1771.135957	322246.533583	37.398272
1772.808443	322836.354364	37.403290
1774.690106	323426.693947	37.408308
1776.092947	324022.845493	37.413325
1778.227667	324617.626652	37.418343
1779.969085	325217.494444	37.423360
1781.664655	325814.088785	37.428378
1783.721369	326414.020115	37.433396
1785.100666	327030.281376	37.438413
1786.671345	327618.398850	37.443431
1788.524909	328247.111987	37.448448
1790.212853	328856.448812	37.453466
1792.238654	329479.357383	37.458484
1793.663203	330114.748103	37.463501
1795.453811	330732.756917	37.468519
1797.015024	331366.994425	37.473536
1798.650413	332009.565219	37.478554
1800.315337	332646.132543	37.483572
1801.754778	333290.041355	37.488589
1803.610622	333950.730823	37.493607
1805.048996	334613.740704	37.498624
1806.926883	335277.685562	37.503642
1809.216413	335935.741130	37.508660
1810.700782	336601.029442	37.513677
1812.841494	337267.343580	37.518695
1814.748003	337930.768771	37.523712
1816.377553	338605.705083	37.528730
1818.221727	339280.140380	37.533748
1820.159851	339952.013038	37.538765
1821.993004	340625.366482	37.543783
1823.852350	341310.941380	37.548800
1825.483876	341989.488162	37.553818
1827.895544	342659.774705	37.558836
1829.418911	343345.631051	37.563853
1831.404431	344024.447040	37.568871
1833.075476	344696.554046	37.573888
1835.239696	345378.570517	37.578906
1837.517513	346053.655052	37.583924
1839.039459	346749.438149	37.588941
1841.246538	347412.129499	37.593959
1843.089427	348085.048791	37.598976
1845.071308	348765.879140	37.603994
1847.054750	349431.725715	37.609012
1849.289890	350105.921391	37.614029
1851.062787	350780.716288	37.619047
1852.775528	351452.668745	37.624064
1854.499775	352127.756042	37.629082
1856.875405	352792.803291	37.634100
1858.362400	353464.026748	37.639117
1860.325965	354138.206483	37.644135
1862.140434	354802.985984	37.649152
1863.851892	355474.902755	37.654170
1865.753038	356153.019986	37.659188
1867.590470	356824.158949	37.664205
1869.951145	357491.699346	37.669223
1871.551850	358166.586039	37.674240
1872.970997	358827.206587	37.679258
1875.112918	359482.851172	37.684276
1877.133535	360128.686164	37.689293
1878.785868	360777.058198	37.694311
1880.748509	361412.784331	37.699328
1882.306016	362069.422557	37.704346
1884.155900	362720.217256	37.709364
1885.503390	363395.110101	37.714381
1887.597077	364049.597687	37.719399
1889.235945	364714.474881	37.724416
1890.762985	365397.878769	37.729434
1892.652742	366058.987778	37.734452
1894.353013	366753.197052	37.739469
1896.512385	367438.921289	37.744487
1898.348398	368132.930950	37.749504
1899.951517	368838.964886	37.754522
1901.971648	369527.591509	37.759540
1904.203253	370225.936490	37.764557
1905.450796	370933.181773	37.769575
1907.240955	371633.602288	37.774592
1909.356359	372344.558172	37.779610
1911.739200	373065.931434	37.784628
1913.534741	373773.107535	37.789645
1915.944892	374488.893259	37.794663
1918.163069	375202.794138	37.799680
1919.957607	375908.888333	37.804698
1921.674289	376606.104731	37.809716
1924.086526	377323.887147	37.814733
1926.352016	378046.066369	37.819751
1928.112052	378734.154061	37.824768
1930.273199	379438.087605	37.829786
1932.434373	380146.393783	37.834804
1934.535965	380864.635554	37.839821
1936.209231	381574.590008	37.844839
1938.313379	382281.871977	37.849856
1940.005214	382988.395590	37.854874
1941.637405	383709.443167	37.859892
1943.531940	384427.059455	37.864909
1945.537465	385156.736172	37.869927
1947.417519	385881.853478	37.874944
1949.112665	386619.484620	37.879962
1951.262486	387352.840621	37.884980
1952.803977	388083.111110	37.889997
1954.889790	388817.154018	37.895015
1957.574830	389554.402187	37.900032
1959.258933	390295.423424	37.905050
1961.432717	391018.170121	37.910068
1963.176591	391776.334050	37.915085
1964.866424	392514.690612	37.920103
1966.916883	393248.838198	37.925120
1968.429953	394006.503772	37.930138
1970.734238	394749.850842	37.935156
1972.509956	395507.131552	37.940173
1974.337362	396274.472481	37.945191
1976.126061	397026.542186	37.950208
1977.868650	397796.519326	37.955226
1980.121837	398555.139450	37.960244
1981.822663	399324.855585	37.965261
1984.204661	400102.802306	37.970279
1986.010423	400863.970768	37.975296
1987.998858	401643.461707	37.980314
1989.828229	402402.862545	37.985332
1991.858257	403179.593517	37.990349
1993.875155	403969.405987	37.995367
1995.622293	404737.981759	38.000384
1997.151282	405521.699381	38.005402
1999.039478	406327.860742	38.010420
2001.384636	407112.792734	38.015437
2003.132967	407896.534156	38.020455
2005.411052	408668.613120	38.025472
2007.118081	409450.011620	38.030490
2009.229814	410223.568896	38.035508
2011.365832	410982.432325	38.040525
2012.942745	411769.460155	38.045543
2015.147957	412537.463996	38.050560
2016.958213	413311.286342	38.055578
2019.010600	414087.148644	38.060596
2021.282318	414871.260047	38.065613
2022.849694	415665.114442	38.070631
2025.342177	416454.157224	38.075648
2027.876564	417230.505689	38.080666
2030.112216	417990.190154	38.085684
2032.236488	418775.398750	38.090701
2034.123158	419561.382257	38.095719
2036.504775	420340.143919	38.100736
2038.327688	421142.296505	38.105754
2040.608908	421914.163792	38.110772
2042.496323	422704.633084	38.115789
2044.350328	423508.528270	38.120807
2046.068380	424313.356780	38.125824
2048.207802	425115.380524	38.130842
2049.994233	425928.981555	38.135860
2052.064603	426736.128791	38.140877
2054.388641	427540.372056	38.145895
2056.447382	428344.733720	38.150912
2058.649608	429179.119108	38.155930
2060.004462	429987.794980	38.160948
2062.447672	430826.285506	38.165965
2063.897946	431648.001663	38.170983
2066.006665	432481.679617	38.176000
2067.984553	433330.485371	38.181018
2070.025648	434181.173541	38.186036
2072.533564	435022.035220	38.191053
2074.441065	435879.972294	38.196071
2076.388503	436730.531990	38.201088
2078.434447	437589.850446	38.206106
2080.282685	438441.982671	38.211124
2082.588269	439313.390436	38.216141
2084.262157	440190.941598	38.221159
2086.575234	441044.974195	38.226176
2088.469847	441932.086437	38.231194
2090.670310	442816.026423	38.236212
2092.692871	443691.763731	38.241229
2094.302056	444573.201295	38.246247
2096.875449	445469.319177	38.251264
2098.859471	446362.563266	38.256282
2100.682894	447263.385703	38.261300
2103.478579	448145.748257	38.266317
2105.697428	449039.349279	38.271335
2107.867404	449922.450412	38.276352
2110.195511	450819.297710	38.281370
2112.427310	451704.135807	38.286388
2114.577658	452595.019620	38.291405
2116.434358	453493.247576	38.296423
2118.647672	454386.472703	38.301440
2120.611042	455281.268524	38.306458
2122.724622	456168.365208	38.311476
2125.041330	457069.751174	38.316493
2127.048131	457970.036368	38.321511
2129.353141	458855.974394	38.326528
2131.502184	459770.162487	38.331546
2133.656231	460655.490904	38.336564
2136.024476	461543.778524	38.341581
2137.825882	462450.016118	38.346599
2140.249357	463343.017521	38.351616
2142.464185	464234.143036	38.356634
2144.868243	465124.691871	38.361652
2147.367934	465984.555229	38.366669
2149.693934	466831.925847	38.371687
2151.778178	467683.342834	38.376704
2154.450030	468531.391375	38.381722
2156.080012	469376.946868	38.386740
2158.321325	470217.311310	38.391757
2160.274086	471079.566447	38.396775
2162.199738	471932.338498	38.401792
2164.142191	472802.955952	38.406810
2165.813647	473674.740301	38.411828
2167.970596	474539.078874	38.416845
2169.832521	475426.917872	38.421863
2171.659983	476314.063881	38.426880
2173.533289	477211.919799	38.431898
2175.368484	478109.031563	38.436916
2177.838140	479017.460938	38.441933
2179.563370	479938.746607	38.446951
2181.696494	480846.282710	38.451968
2184.079716	481769.842660	38.456986
2186.499380	482702.540666	38.462004
2189.635579	483610.682739	38.467021
2191.914159	484553.054567	38.472039
2194.732483	485458.580811	38.477056
2197.275336	486388.341376	38.482074
2198.963857	487310.469992	38.487092
2201.402164	488219.250919	38.492109
2202.660180	489156.045315	38.497127
2204.904784	490071.678766	38.502144
2207.256149	491020.510295	38.507162
2208.985540	491969.342406	38.512180
2211.541483	492902.946416	38.517197
2213.199640	493858.803353	38.522215
2215.353958	494827.192149	38.527232
2217.300598	495787.133529	38.532250
2219.257549	496768.060699	38.537268
2221.677283	497744.364527	38.542285
2223.661404	498729.614185	38.547303
2226.139188	499696.310734	38.552320
2228.481997	500682.295246	38.557338
2230.134599	501678.676583	38.562356
2232.644794	502668.703203	38.567373
2234.806726	503670.278559	38.572391
2236.985394	504669.369634	38.577408
2239.325671	505676.593866	38.582426
2241.424428	506688.990234	38.587444
2244.056516	507681.469037	38.592461
2246.530549	508685.157574	38.597479
2249.150904	509679.079237	38.602496
2251.496103	510687.303261	38.607514
2254.153405	511688.505927	38.612532
2256.574068	512667.806962	38.617549
2258.941416	513670.848670	38.622567
2261.521434	514664.164778	38.627584
2263.885152	515646.970772	38.632602
2266.198050	516637.434578	38.637620
2268.690277	517613.040702	38.642637
2271.121199	518601.193747	38.647655
2273.237158	519579.107180	38.652672
2276.003836	520563.048905	38.657690
2278.156609	521537.910035	38.662708
2280.219229	522513.177598	38.667725
2282.579031	523495.688800	38.672743
2284.711664	524470.668746	38.677760
2287.303537	525455.281910	38.682778
2288.957710	526436.661496	38.687796
2291.560128	527418.223752	38.692813
2293.749683	528406.739416	38.697831
2295.935518	529381.695119	38.702848
2297.784577	530333.732321	38.707866
2300.036241	531304.875401	38.712884
2302.334209	532257.067470	38.717901
2304.337410	533219.617148	38.722919
2306.417478	534188.433779	38.727936
2308.533321	535158.942103	38.732954
2310.865723	536129.299767	38.737972
2313.137017	537109.769112	38.742989
2315.122947	538097.969190	38.748007
2317.338611	539082.088202	38.753024
2319.552306	540079.776435	38.758042
2321.331371	541091.202757	38.763060
2323.554755	542106.056171	38.768077
2326.191578	543126.805823	38.773095
2328.045959	544155.558869	38.778112
2330.790595	545170.609517	38.783130
2332.971038	546204.993764	38.788148
2335.300619	547243.501541	38.793165
2337.885720	548286.516396	38.798183
2339.604763	549327.181955	38.803200
2342.189007	550370.995434	38.808218
2344.511859	551440.867103	38.813236
2346.876647	552503.610104	38.818253
2349.030467	553567.310665	38.823271
2351.231967	554643.989445	38.828288
2353.870294	555716.339009	38.833306
2356.093825	556811.589491	38.838324
2358.530134	557896.665015	38.843341
2361.026444	558970.889382	38.848359
2363.517219	560067.990580	38.853376
2365.992769	561160.230889	38.858394
2367.647156	562256.485341	38.863412
2370.083608	563356.940395	38.868429
2372.347786	564454.569198	38.873447
2374.457482	565580.207176	38.878464
2377.184753	566697.359921	38.883482
2379.500577	567827.390041	38.888500
2382.110705	568951.699570	38.893517
2384.756332	570081.578699	38.898535
2387.097138	571198.607030	38.903552
2389.832502	572328.072687	38.908570
2392.393996	573451.443713	38.913588
2394.937212	574567.290381	38.918605
2397.379920	575698.662842	38.923623
2400.011574	576827.243088	38.928640
2402.169828	577935.177606	38.933658
2404.561733	579061.488901	38.938676
2407.025766	580197.469166	38.943693
2409.427523	581325.530478	38.948711
2411.567852	582447.462968	38.953728
2414.100301	583591.446681	38.958746
2416.799301	584725.467275	38.963764
2419.241540	585855.513888	38.968781
2421.626981	586997.999984	38.973799
2423.725484	588141.228102	38.978816
2426.714601	589270.766620	38.983834
2428.711692	590410.839036	38.988852
2431.207566	591544.405892	38.993869
2434.482411	592683.851104	38.998887
2437.320031	593815.091451	39.003904
2440.597034	594922.351248	39.008922
2442.910589	596047.101642	39.013940
2445.307494	597155.149086	39.018957
2447.822718	598258.313873	39.023975
2449.902089	599377.174060	39.028992
2452.623865	600495.270239	39.034010
2454.256170	601608.781354	39.039028
2456.437561	602722.145115	39.044045
2459.237390	603821.530948	39.049063
2461.350688	604912.163910	39.054080
2463.868116	605994.867534	39.059098
2465.911193	607092.713162	39.064116
2468.357980	608183.279563	39.069133
2471.132902	609275.789034	39.074151
2473.087048	610388.844481	39.079168
2475.605289	611485.936350	39.084186
2477.439758	612606.097469	39.089204
2480.188825	613725.795783	39.094221
2482.600148	614850.789586	39.099239
2484.589005	615979.790491	39.104256
2486.978793	617122.813002	39.109274
2489.068620	618277.367682	39.114292
2491.842248	619421.038952	39.119309
2494.194233	620568.260112	39.124327
2496.461252	621748.517096	39.129344
2499.166445	622915.928493	39.134362
2501.378293	624094.690588	39.139380
2503.912349	625279.617661	39.144397
2506.463568	626467.959375	39.149415
2508.709983	627670.258937	39.154432
2511.701389	628864.407882	39.159450
2514.336122	630057.433099	39.164468
2517.032126	631256.907014	39.169485
2519.901976	632453.370082	39.174503
2522.194770	633652.588981	39.179520
2525.259565	634856.486784	39.184538
2528.117633	636062.027732	39.189556
2530.586964	637253.367706	39.194573
2532.939003	638457.816839	39.199591
2535.293595	639669.012556	39.204608
2537.978083	640866.739276	39.209626
2540.407602	642085.173903	39.214644
2542.793490	643319.384915	39.219661
2545.075852	644539.348186	39.224679
2547.491021	645774.255575	39.229696
2550.159806	647007.724500	39.234714
2553.274912	648248.199687	39.239732
2555.730174	649481.152878	39.244749
2558.838752	650702.232347	39.249767
2561.571530	651945.654682	39.254784
2564.328364	653161.806811	39.259802
2567.131485	654389.313852	39.264820
2569.820053	655612.303362	39.269837
2572.559907	656834.535399	39.274855
2574.703219	658071.707892	39.279872
2577.506056	659290.137713	39.284890
2580.253414	660521.871160	39.289908
2582.108708	661762.409730	39.294925
2584.895176	662996.512759	39.299943
2587.162075	664231.987978	39.304960
2589.442037	665482.932376	39.309978
2592.062198	666732.214920	39.314996
2594.281349	667985.779975	39.320013
2597.239686	669240.800338	39.325031
2599.459850	670500.453499	39.330048
2602.253214	671767.405965	39.335066
2605.309140	673032.504333	39.340084
2607.242491	674289.910141	39.345101
2610.181446	675554.042634	39.350119
2612.196063	676829.392630	39.355136
2615.215303	678097.443740	39.360154
2617.816787	679370.261739	39.365172
2620.362411	680656.282254	39.370189
2623.291223	681909.366057	39.375207
2625.524866	683205.368297	39.380224
2628.407216	684464.818627	39.385242
2631.195030	685713.035420	39.390260
2633.414931	686959.387282	39.395277
2636.334470	688184.201171	39.400295
2638.714223	689426.960496	39.405312
2641.302124	690662.465695	39.410330
2643.571488	691902.320968	39.415348
2646.495862	693168.050329	39.420365
2649.204826	694399.001706	39.425383
2651.813660	695665.124031	39.430400
2654.364359	696922.245889	39.435418
2656.836090	698184.410345	39.440436
2659.206799	699451.767050	39.445453
2662.180268	700724.990513	39.450471
2664.446585	702006.623540	39.455488
2666.981061	703292.337252	39.460506
2669.447235	704585.901820	39.465524
2672.106645	705898.122510	39.470541
2674.966974	707195.792185	39.475559
2677.576458	708509.705951	39.480576
2680.058576	709811.601954	39.485594
2683.020336	711139.568577	39.490612
2685.416222	712469.105841	39.495629
2688.263805	713793.410383	39.500647
2690.944240	715137.089150	39.505664
2693.413305	716480.639048	39.510682
2696.056570	717831.171285	39.515700
2698.141050	719177.472153	39.520717
2700.978905	720530.803702	39.525735
2703.692675	721916.136036	39.530752
2706.228138	723290.981037	39.535770
2708.761437	724670.493750	39.540788
2711.605771	726077.063702	39.545805
2714.207016	727466.776405	39.550823
2717.012931	728875.938880	39.555840
2719.702362	730266.941716	39.560858
2722.277090	731684.305151	39.565876
2725.309799	733094.727289	39.570893
2728.687156	734496.945483	39.575911
2731.121153	735916.851476	39.580928
2733.994274	737321.574826	39.585946
2737.233471	738730.286219	39.590964
2739.698782	740151.412128	39.595981
2742.785568	741566.310524	39.600999
2745.294491	742981.940115	39.606016
2748.352094	744385.930841	39.611034
2751.152433	745804.360913	39.616052
2753.977660	747231.455576	39.621069
2756.835797	748644.185801	39.626087
2759.461300	750066.310213	39.631104
2762.215503	751481.205208	39.636122
2765.538288	752900.035092	39.641140
2768.307386	754318.400351	39.646157
2770.652062	755733.274661	39.651175
2773.601010	757164.925661	39.656192
2776.313025	758584.039465	39.661210
2779.654359	759993.728269	39.666228
2781.824101	761419.442607	39.671245
2784.773099	762844.809726	39.676263
2787.950933	764269.427552	39.681280
2790.297673	765689.141670	39.686298
2793.298184	767128.052860	39.691316
2795.584030	768557.561344	39.696333
2798.346107	769987.553182	39.701351
2801.106918	771412.748389	39.706368
2804.134344	772841.851751	39.711386
2807.036275	774272.517208	39.716404
2810.106027	775723.311768	39.721421
2813.389071	777125.359708	39.726439
2816.038048	778517.717455	39.731456
2818.829006	779894.812425	39.736474
2821.860979	781267.876446	39.741492
2824.631074	782638.956816	39.746509
2827.392407	784011.397673	39.751527
2829.655982	785398.621333	39.756544
2832.929382	786776.974599	39.761562
2835.883724	788159.724604	39.766580
2838.441802	789551.097082	39.771597
2841.391424	790927.084362	39.776615
2844.171853	792330.179570	39.781632
2846.839716	793718.756255	39.786650
2849.767557	795114.267081	39.791668
2852.312795	796523.474110	39.796685
2855.336505	797938.342194	39.801703
2857.815707	799356.342699	39.806720
2860.343837	800782.661588	39.811738
2863.393067	802206.790830	39.816756
2865.748636	803654.325313	39.821773
2868.685067	805099.307964	39.826791
2871.186031	806562.790825	39.831808
2873.697028	808037.646319	39.836826
2876.454174	809510.725243	39.841844
2879.108307	811004.812948	39.846861
2881.869006	812498.065699	39.851879
2884.745589	814003.183734	39.856896
2887.498621	815511.845046	39.861914
2890.473772	817035.367276	39.866932
2893.007184	818565.353446	39.871949
2895.305244	820098.932912	39.876967
2898.055517	821644.528597	39.881984
2900.788618	823206.989370	39.887002
2904.224471	824757.307743	39.892020
2907.063631	826339.203344	39.897037
2910.064340	827916.303757	39.902055
2913.694916	829486.145565	39.907072
2916.523165	831058.129745	39.912090
2919.597291	832628.719242	39.917108
2922.135909	834216.891640	39.922125
2925.801581	835776.391657	39.927143
2929.513523	837339.741806	39.932160
2932.205339	838912.808082	39.937178
2935.162578	840482.037886	39.942196
2938.387183	842059.788507	39.947213
2941.015289	843621.147904	39.952231
2944.569128	845197.383351	39.957248
2946.723945	846787.844488	39.962266
2950.039591	848358.856683	39.967284
2952.809628	849943.266564	39.972301
2955.982793	851521.379876	39.977319
2958.901081	853091.754411	39.982336
2962.160739	854666.530704	39.987354
2965.034908	856250.677357	39.992372
2967.966371	857837.222466	39.997389
2970.492758	859410.424251	40.002407
2973.871721	861001.996622	40.007424
2976.818784	862603.310895	40.012442
2979.947121	864188.275274	40.017460
2982.835161	865782.363951	40.022477
2985.695143	867367.704513	40.027495
2988.467973	868959.036429	40.032512
2991.390850	870553.699610	40.037530
2994.289972	872150.653534	40.042548
2996.848147	873764.466040	40.047565
3000.079632	875381.988187	40.052583
3003.164177	876988.452510	40.057600
3005.661584	878603.281761	40.062618
3008.560178	880215.282449	40.067636
3011.543221	881793.769324	40.072653
3014.449308	883367.012058	40.077671
3017.476580	884946.380664	40.082688
3019.825799	886546.874077	40.087706
3022.747333	888120.472300	40.092724
3025.411610	889715.114695	40.097741
3028.532025	891314.838395	40.102759
3031.357034	892916.963596	40.107776
3034.261891	894536.470945	40.112794
3037.240364	896160.039011	40.117812
3040.306950	897789.780971	40.122829
3043.088431	899427.100475	40.127847
3046.001189	901060.167534	40.132864
3049.223680	902720.833251	40.137882
3052.575971	904366.833812	40.142900
3054.869387	906025.134525	40.147917
3058.047148	907706.468429	40.152935
3061.302886	909380.740570	40.157952
3064.113147	911074.198757	40.162970
3067.377722	912751.297404	40.167988
3070.328157	914459.076156	40.173005
3073.325042	916159.399040	40.178023
3076.780728	917861.999887	40.183040
3079.837650	919575.753355	40.188058
3082.689877	921285.449267	40.193076
3085.838545	923009.814281	40.198093
3089.075189	924734.765736	40.203111
3092.195771	926468.773325	40.208128
3094.765892	928211.993686	40.213146
3097.650188	929942.711287	40.218164
3101.036898	931681.981288	40.223181
3104.066251	933453.206562	40.228199
3107.144217	935215.023807	40.233216
3109.865403	936974.684864	40.238234
3113.232071	938750.106726	40.243252
3116.181082	940531.308420	40.248269
3119.145523	942320.505058	40.253287
3122.391530	944104.070760	40.258304
3125.160031	945911.465116	40.263322
3128.520567	947699.506425	40.268340
3131.894019	949497.427501	40.273357
3134.851392	951311.680813	40.278375
3138.065809	953117.139254	40.283392
3141.236420	954941.587388	40.288410
3144.386419	956800.993364	40.293428
3147.477671	958675.653445	40.298445
3150.644538	960557.317674	40.303463
3154.082167	962409.784994	40.308480
3156.864471	964283.845123	40.313498
3160.126315	966161.708856	40.318516
3163.713239	968048.571917	40.323533
3166.695155	969935.110128	40.328551
3169.890663	971799.331762	40.333568
3173.092104	973684.015570	40.338586
3176.273981	975569.837915	40.343604
3179.689063	977435.895023	40.348621
3182.729953	979324.304854	40.353639
3186.269531	981200.026720	40.358656
3189.185526	983089.745049	40.363674
3192.132802	984979.416467	40.368692
3195.228741	986883.326524	40.373709
3198.522145	988781.606129	40.378727
3201.555604	990673.654702	40.383744
3204.380573	992570.066211	40.388762
3207.273876	994481.286150	40.393780
3210.510154	996393.749123	40.398797
3213.172127	998317.996109	40.403815
3216.640569	1000237.573230	40.408832
3219.394307	1002128.568044	40.413850
3222.580015	1004014.978533	40.418868
3225.968712	1005894.615375	40.423885
3228.598096	1007779.956837	40.428903
3231.789456	1009679.405333	40.433920
3234.734964	1011568.758580	40.438938
3237.760753	1013472.768694	40.443956
3241.237025	1015399.298888	40.448973
3244.054558	1017316.178557	40.453991
3247.568954	1019237.707805	40.459008
3250.430872	1021164.490111	40.464026
3253.999396	1023102.387244	40.469044
3257.752217	1025045.963071	40.474061
3261.078066	1026983.426296	40.479079
3264.703175	1028922.776786	40.484096
3267.720302	1030876.424304	40.489114
3271.061373	1032819.971421	40.494132
3274.530374	1034784.241325	40.499149
3277.570851	1036745.959910	40.504167
3280.820832	1038707.434582	40.509184
3283.894779	1040683.572331	40.514202
3286.699518	1042685.838328	40.519220
3289.907407	1044665.258006	40.524237
3293.243146	1046661.955532	40.529255
3296.308377	1048675.014380	40.534272
3299.705999	1050696.234316	40.539290
3302.789725	1052705.032854	40.544308
3305.806452	1054733.687133	40.549325
3308.888444	1056789.072454	40.554343
3312.323627	1058830.278902	40.559360
3315.433802	1060889.221767	40.564378
3318.734218	1062950.146883	40.569396
3321.933225	1065006.477277	40.574413
3325.184400	1067094.741343	40.579431
3328.764010	1069172.183408	40.584448
3332.094299	1071264.120322	40.589466
3335.076623	1073350.811640	40.594484
3338.248817	1075446.924498	40.599501
3341.478994	1077571.713770	40.604519
3345.120032	1079670.053773	40.609536
3348.286074	1081784.120250	40.614554
3351.620035	1083898.199364	40.619572
3355.340354	1086021.048994	40.624589
3358.433089	1088160.278381	40.629607
3362.042553	1090276.705208	40.634624
3365.568412	1092419.247170	40.639642
3368.755613	1094557.657211	40.644660
3372.417146	1096692.568460	40.649677
3375.672490	1098823.270443	40.654695
3378.789026	1100943.049511	40.659712
3382.363174	1103103.946918	40.664730
3385.599471	1105258.127869	40.669748
3389.000792	1107407.325615	40.674765
3391.769112	1109564.240440	40.679783
3394.673291	1111727.403281	40.684800
3398.208740	1113896.913921	40.689818
3401.860943	1116072.657870	40.694836
3405.144807	1118246.723707	40.699853
3408.309986	1120439.019058	40.704871
3411.747042	1122610.905803	40.709888
3415.126102	1124803.653900	40.714906
3418.518736	1126997.206325	40.719924
3422.130907	1129176.637836	40.724941
3425.198203	1131382.378390	40.729959
3428.046581	1133585.629403	40.734976
3431.714469	1135790.105001	40.739994
3434.778044	1137998.687587	40.745012
3438.321064	1140180.368192	40.750016
3441.479543	1142334.612008	40.755021
3444.533824	1144422.202110	40.760026
3447.707082	1146448.391732	40.765031
3450.797412	1148407.410251	40.770036
3454.322250	1150292.049181	40.775040
3457.378778	1152103.388008	40.780045
3460.616405	1153811.206089	40.785050
3463.274790	1155449.219323	40.790055
3465.863734	1157029.325253	40.795060
3468.908009	1158512.345330	40.800064
3471.542593	1159931.587691	40.805069
3474.179988	1161257.362526	40.810074
3476.659036	1162515.654154	40.815079
3478.558179	1163692.884083	40.820084
3481.211470	1164809.663333	40.825088
3483.138837	1165864.102480	40.830093
3485.010855	1166837.248634	40.835098
3486.555635	1167751.749676	40.840103
3488.379986	1168604.516591	40.845108
3490.388222	1169412.295954	40.850112
3491.993946	1170156.054044	40.855117
3493.560957	1170847.266328	40.860122
3495.196847	1171480.276939	40.865127
3496.023532	1172073.924237	40.870132
3497.662091	1172619.185192	40.875136
3498.849428	1173120.525860	40.880141
3499.822946	1173578.768333	40.885146
3500.749661	1173998.987114	40.890151
3501.800734	1174385.876410	40.895156
3503.477131	1174727.013381	40.900160
3503.989524	1175052.296863	40.905165
3504.852984	1175316.147674	40.910170
3505.693211	1175559.915265	40.915175
3506.254368	1175791.372153	40.920180
3507.412880	1175983.801439	40.925184
3507.819110	1176151.941460	40.930189
3508.640871	1176277.133267	40.935194
3509.339938	1176396.500156	40.940199
3510.026814	1176476.103043	40.945204
3510.750193	1176549.479866	40.950208
3510.963030	1176592.505469	40.955213
3511.855070	1176621.379582	40.960218
3512.000518	1176624.182442	40.965223
3512.591574	1176615.039757	40.970228
3513.511273	1176583.040736	40.975232
3513.771407	1176537.393313	40.980237
3514.148527	1176475.802037	40.985242
3514.741388	1176387.696589	40.990247
3515.217425	1176290.751330	40.995252
3515.703643	1176176.746716	41.000256
3515.711174	1176062.629974	41.005261
3516.186605	1175911.964349	41.010266
3516.473179	1175762.456336	41.015271
3516.730892	1175610.215773	41.020276
3516.982323	1175427.247988	41.025280
3517.369791	1175250.189015	41.030285
3517.461450	1175065.538364	41.035290
3517.929945	1174860.271478	41.040295
3517.909596	1174661.769401	41.045300
3518.546711	1174440.528423	41.050304
3518.193517	1174209.731640	41.055309
3518.236406	1173988.380786	41.060314
3518.875286	1173747.124558	41.065319
3518.752026	1173500.703006	41.070324
3518.981916	1173255.814470	41.075328
3518.867067	1172997.959330	41.080333
3519.195663	1172732.757777	41.085338
3519.206015	1172462.220120	41.090343
3519.106115	1172211.490302	41.095348
3519.484972	1171929.359291	41.100352
3519.586799	1171658.953501	41.105357
3519.822784	1171367.855878	41.110362
3519.895299	1171074.788131	41.115367
3519.548461	1170792.809477	41.120372
3519.949954	1170499.938243	41.125376
3519.705581	1170206.024867	41.130381
3520.089992	1169899.443498	41.135386
3520.271923	1169603.539082	41.140391
3520.127903	1169312.011937	41.145396
3520.506374	1168988.582718	41.150400
3520.598371	1168672.541302	41.155405
3520.578710	1168358.480980	41.160410
3520.650779	1168035.986962	41.165415
3520.415217	1167709.748314	41.170420
3520.372765	1167380.814551	41.175424
3520.350535	1167071.302400	41.180429
3520.525349	1166742.009458	41.185434
3520.585820	1166410.259996	41.190439
3520.591898	1166089.922534	41.195444
3520.608241	1165749.452324	41.200448
3520.760614	1165411.298200	41.205453
3520.570254	1165078.089135	41.210458
3520.878376	1164748.365398	41.215463
3520.691119	1164412.091382	41.220468
3520.749211	1164058.754272	41.225472
3520.732573	1163735.537295	41.230477
3520.968289	1163381.369559	41.235482
3521.245963	1163038.885126	41.240487
3520.763366	1162697.920633	41.245492
3521.248275	1162342.129979	41.250496
3520.720748	1161993.662984	41.255501
3520.510440	1161653.058057	41.260506
3520.847818	1161302.890771	41.265511
3520.823814	1160951.247505	41.270516
3520.903754	1160588.694530	41.275520
3520.996924	1160250.594848	41.280525
3520.914982	1159900.686526	41.285530
3521.202894	1159541.051689	41.290535
3520.954719	1159191.407022	41.295540
3520.992397	1158822.215741	41.300544
3520.749022	1158466.281984	41.305549
3520.475608	1158119.217456	41.310554
3520.498161	1157770.000827	41.315559
3520.473348	1157415.661975	41.320564
3520.570506	1157057.779785	41.325568
3520.765815	1156720.665312	41.330573
3520.497511	1156361.282530	41.335578
3520.977859	1156000.616715	41.340583
3520.879269	1155649.765526	41.345588
3520.850464	1155293.297520	41.350592
3520.496070	1154936.102041	41.355597
3520.587873	1154559.506004	41.360602
3521.044566	1154203.925021	41.365607
3520.747715	1153859.989506	41.370612
3520.695119	1153483.624118	41.375616
3520.626147	1153127.489105	41.380621
3520.748592	1152771.866387	41.385626
3520.597529	1152407.934574	41.390631
3520.350956	1152033.958616	41.395636
3520.260717	1151676.024879	41.400640
3520.487365	1151318.582703	41.405645
3520.244902	1150972.082460	41.410650
3520.237044	1150615.293986	41.415655
3520.232049	1150257.439188	41.420660
3520.599908	1149896.089284	41.425664
3520.219369	1149530.102260	41.430669
3520.175090	1149182.693999	41.435674
3520.794943	1148816.113781	41.440679
3520.285640	1148454.809556	41.445684
3520.835231	1148089.990351	41.450688
3520.320009	1147742.564776	41.455693
3520.346161	1147372.855488	41.460698
3520.483811	1147001.396301	41.465703
3520.324190	1146644.553605	41.470708
3520.251300	1146281.607191	41.475712
3520.378176	1145930.070933	41.480717
3520.039266	1145556.313907	41.485722
3520.207887	1145197.802834	41.490727
3519.784212	1144839.933757	41.495732
3520.114615	1144491.491316	41.500736
3520.074976	1144126.590080	41.505741
3519.689060	1143767.788881	41.510746
3519.859580	1143422.431216	41.515751
3519.740032	1143069.986663	41.520756
3519.766285	1142699.476033	41.525760
3519.631395	1142354.573104	41.530765
3519.653026	1142003.172299	41.535770
3519.978789	1141626.751529	41.540775
3519.582165	1141276.983900	41.545780
3519.866245	1140913.989446	41.550784
3519.647504	1140548.586213	41.555789
3519.343455	1140198.257682	41.560794
3519.587536	1139857.588932	41.565799
3519.406273	1139500.836697	41.570804
3519.567645	1139134.988643	41.575808
3519.584052	1138789.543780	41.580813
3519.272482	1138437.201905	41.585818
3519.808625	1138081.944385	41.590823
3519.233865	1137733.490688	41.595828
3519.052872	1137371.753948	41.600832
3519.049180	1137017.178511	41.605837
3518.524149	1136676.811701	41.610842
3518.598336	1136326.924424	41.615847
3518.634185	1135992.593013	41.620852
3519.339536	1135647.589612	41.625856
3518.942470	1135307.018879	41.630861
3518.998354	1134951.820766	41.635866
3518.970228	1134607.440419	41.640871
3518.860719	1134270.555015	41.645876
3518.792570	1133912.553226	41.650880
3518.880558	1133566.946382	41.655885
3518.681624	1133221.934337	41.660890
3518.883259	1132870.658224	41.665895
3518.584475	1132530.368255	41.670900
3518.600117	1132193.615582	41.675904
3518.762675	1131845.603967	41.680909
3518.779330	1131500.444665	41.685914
3518.814087	1131148.797164	41.690919
3518.564929	1130821.980584	41.695924
3518.132370	1130471.410783	41.700928
3518.369601	1130136.867717	41.705933
3518.486129	1129797.094898	41.710938
3518.678261	1129453.675214	41.715943
3518.234082	1129113.190510	41.720948
3518.613648	1128758.951343	41.725952
3518.597840	1128437.464764	41.730957
3518.199079	1128083.784326	41.735962
3518.545096	1127743.081874	41.740967
3518.265524	1127398.561226	41.745972
3518.257337	1127054.734520	41.750976
3518.258087	1126718.303574	41.755981
3518.082457	1126387.397783	41.760986
3518.507833	1126043.244183	41.765991
3518.126544	1125705.956079	41.770996
3518.245455	1125365.519627	41.776000
3518.195561	1125021.092916	41.781005
3517.958593	1124684.001863	41.786010
3518.306749	1124338.418804	41.791015
3517.820518	1124012.270104	41.796020
3517.944601	1123670.868157	41.801024
3518.056107	1123337.727196	41.806029
3517.953279	1122992.702383	41.811034
3518.094998	1122653.041012	41.816039
3517.885665	1122322.174172	41.821044
3517.943852	1121981.817486	41.826048
3517.728682	1121651.290875	41.831053
3517.587927	1121328.729769	41.836058
3517.740970	1120986.961063	41.841063
3517.699659	1120647.202323	41.846068
3517.548720	1120313.249371	41.851072
3517.551328	1119989.060057	41.856077
3517.512176	1119650.285262	41.861082
3517.775084	1119307.914916	41.866087
3517.178057	1118995.575459	41.871092
3517.540557	1118661.625336	41.876096
3517.496257	1118336.867301	41.881101
3516.671403	1118002.023597	41.886106
3517.129358	1117677.523943	41.891111
3516.821465	1117355.989384	41.896116
3517.265868	1117041.553889	41.901120
3517.370181	1116718.007279	41.906125
3517.106480	1116390.689555	41.911130
3516.928984	1116058.381487	41.916135
3516.771724	1115734.341996	41.921140
3516.887488	1115423.868977	41.926144
3516.989382	1115099.081146	41.931149
3516.860595	1114778.029630	41.936154
3517.139464	1114457.273105	41.941159
3516.658795	1114131.569220	41.946164
3516.533639	1113816.466247	41.951168
3516.669152	1113501.587900	41.956173
3516.352293	1113182.855753	41.961178
3516.564746	1112866.878511	41.966183
3516.624486	1112548.714243	41.971188
3516.632990	1112226.724413	41.976192
3516.552960	1111915.222117	41.981197
3516.404331	1111606.574735	41.986202
3516.406198	1111287.772933	41.991207
3516.310262	1110984.995651	41.996212
3516.489243	1110668.703755	42.001216
3516.253760	1110346.736783	42.006221
3515.777549	1110041.774488	42.011226
3516.418543	1109733.366506	42.016231
3515.970291	1109436.094480	42.021236
3516.035898	1109118.203149	42.026240
3516.571049	1108815.104227	42.031245
3516.274956	1108500.576324	42.036250
3516.022169	1108189.459100	42.041255
3516.030138	1107896.417507	42.046260
3515.988167	1107577.307343	42.051264
3515.929665	1107276.701506	42.056269
3515.766429	1106964.353077	42.061274
3515.854814	1106667.889809	42.066279
3515.974235	1106363.002632	42.071284
3515.976128	1106050.383006	42.076288
3515.900966	1105751.795487	42.081293
3515.723822	1105447.764771	42.086298
3516.036298	1105129.406090	42.091303
3515.408141	1104836.493664	42.096308
3515.822558	1104528.875304	42.101312
3515.851387	1104227.129650	42.106317
3515.611233	1103924.360617	42.111322
3515.692606	1103614.643362	42.116327
3515.516607	1103320.332121	42.121332
3515.625305	1103003.887711	42.126336
3515.475985	1102719.857849	42.131341
3515.358799	1102430.647908	42.136346
3515.461577	1102131.352682	42.141351
3515.109592	1101830.873430	42.146356
3515.447697	1101534.851064	42.151360
3515.343279	1101242.325990	42.156365
3515.179686	1100947.214181	42.161370
3515.395474	1100645.810796	42.166375
3515.433175	1100352.545005	42.171380
3515.446406	1100058.406967	42.176384
3515.502255	1099765.775482	42.181389
3514.969619	1099451.809552	42.186394
3515.050271	1099162.487473	42.191399
3515.134255	1098877.930120	42.196404
3514.762412	1098572.874443	42.201408
3514.743846	1098288.972307	42.206413
3514.676882	1098003.820029	42.211418
3514.725461	1097713.373706	42.216423
3514.351142	1097432.354242	42.221428
3514.645053	1097146.045235	42.226432
3514.537439	1096855.100301	42.231437
3514.419087	1096573.228817	42.236442
3514.656418	1096293.484268	42.241447
3514.460843	1096016.092536	42.246452
3514.934417	1095725.469457	42.251456
3514.789469	1095446.605127	42.256461
3514.331213	1095161.271719	42.261466
3514.552556	1094879.256035	42.266471
3514.197107	1094607.272511	42.271476
3514.447856	1094327.806914	42.276480
3514.457470	1094036.212608	42.281485
3514.112682	1093756.911333	42.286490
3513.985882	1093475.741243	42.291495
3514.115317	1093208.680276	42.296500
3514.046513	1092930.248073	42.301504
3514.251723	1092651.086356	42.306509
3513.807202	1092385.515226	42.311514
3514.262612	1092110.305114	42.316519
3513.956546	1091828.600397	42.321524
3514.155143	1091550.627718	42.326528
3514.230310	1091276.491107	42.331533
3513.988452	1091007.084819	42.336538
3514.062437	1090726.888091	42.341543
3513.657601	1090454.512652	42.346548
3513.488231	1090177.008994	42.351552
3513.855034	1089905.532366	42.356557
3513.754888	1089653.657875	42.361562
3513.451757	1089384.851551	42.366567
3513.784783	1089115.160836	42.371572
3513.885338	1088847.698244	42.376576
3514.012242	1088584.145824	42.381581
3513.618397	1088300.356353	42.386586
3513.669553	1088020.406850	42.391591
3513.594897	1087756.080982	42.396596
3513.628692	1087488.370813	42.401600
3513.662048	1087210.203002	42.406605
3513.285957	1086954.799173	42.411610
3513.550114	1086691.323959	42.416615
3513.681313	1086431.403775	42.421620
3513.283507	1086156.894791	42.426624
3513.381522	1085895.900228	42.431629
3513.223735	1085636.181306	42.436634
3513.449061	1085363.830027	42.441639
3513.146785	1085104.205345	42.446644
3513.243061	1084840.284649	42.451648
3513.311233	1084579.040077	42.456653
3512.894796	1084336.366114	42.461658
3513.410160	1084078.571130	42.466663
3512.845467	1083826.982328	42.471668
3513.119339	1083547.149265	42.476672
3513.592138	1083287.118437	42.481677
3512.990678	1083029.745393	42.486682
3513.103214	1082765.721404	42.491687
3512.752389	1082527.655050	42.496692
3513.329568	1082256.337045	42.501696
3513.270476	1082007.362205	42.506701
3512.850657	1081741.362057	42.511706
3512.949241	1081478.524899	42.516711
3512.882434	1081220.306798	42.521716
3512.934966	1080974.911610	42.526720
3512.927546	1080722.224137	42.531725
3512.708350	1080464.954699	42.536730
3512.672548	1080190.180935	42.541735
3512.464115	1079955.528669	42.546740
3512.427128	1079712.969887	42.551744
3512.792953	1079451.142391	42.556749
3512.707529	1079208.377229	42.561754
3512.856211	1078955.006365	42.566759
3512.577808	1078718.105136	42.571764
3512.331104	1078451.819923	42.576768
3512.239264	1078203.732440	42.581773
3512.290191	1077970.583708	42.586778
3512.377965	1077718.893189	42.591783
3512.195448	1077473.763101	42.596788
3512.281982	1077232.129585	42.601792
3511.997594	1076991.218474	42.606797
3512.221910	1076748.196832	42.611802
3512.323708	1076499.135930	42.616807
3512.188075	1076269.977714	42.621812
3512.224900	1076019.273393	42.626816
3512.479128	1075776.395630	42.631821
3512.091726	1075537.837930	42.636826
3511.984657	1075287.315773	42.641831
3511.881438	1075053.203574	42.646836
3512.270372	1074805.746821	42.651840
3512.113566	1074576.617100	42.656845
3511.730537	1074330.130350	42.661850
3512.070659	1074093.502828	42.666855
3511.844567	1073861.088747	42.671860
3511.608950	1073621.846058	42.676864
3511.690931	1073387.439895	42.681869
3511.951913	1073155.588063	42.686874
3512.072480	1072911.452199	42.691879
3511.581735	1072682.298087	42.696884
3511.406541	1072441.456578	42.701888
3511.661057	1072206.971421	42.706893
3511.468341	1071985.810214	42.711898
3511.559619	1071758.251144	42.716903
3511.311895	1071530.161863	42.721908
3511.397668	1071293.935637	42.726912
3511.650879	1071073.529040	42.731917
3511.511169	1070837.800799	42.736922
3511.582208	1070607.217831	42.741927
3511.417967	1070379.547430	42.746932
3511.213870	1070152.739222	42.751936
3511.337796	1069920.196192	42.756941
3511.148193	1069702.498872	42.761946
3511.357297	1069471.076307	42.766951
3511.244766	1069247.484073	42.771956
3511.279001	1069031.453698	42.776960
3511.269515	1068808.403426	42.781965
3510.870866	1068583.965937	42.786970
3511.301991	1068353.036499	42.791975
3511.350421	1068131.199125	42.796980
3511.371377	1067915.992394	42.801985
3511.380524	1067685.969816	42.806989
3511.086360	1067453.679494	42.811994
3510.967180	1067235.584077	42.816999
3511.156086	1067020.699246	42.822004
3511.263212	1066795.624365	42.827009
3511.169791	1066564.994590	42.832013
3510.864587	1066352.377205	42.837018
3510.845065	1066123.929046	42.842023
3510.864398	1065901.044351	42.847028
3510.563239	1065689.170169	42.852033
3510.660113	1065469.814582	42.857037
3510.591671	1065260.867849	42.862042
3510.868559	1065045.795001	42.867047
3510.791771	1064838.372943	42.872052
3510.965524	1064628.784985	42.877057
3510.705853	1064402.132878	42.882061
3510.711833	1064184.761600	42.887066
3510.340545	1063966.962708	42.892071
3510.254679	1063764.794240	42.897076
3510.392088	1063554.016464	42.902081
3510.135731	1063347.530051	42.907085
3510.165925	1063150.709354	42.912090
3510.319301	1062937.980440	42.917095
3510.556353	1062739.763492	42.922100
3510.449249	1062527.254090	42.927105
3510.647026	1062312.664824	42.932109
3509.872900	1062105.061896	42.937114
3510.286466	1061905.630660	42.942119
3510.487496	1061692.653188	42.947124
3510.163949	1061480.042689	42.952129
3510.293703	1061275.629139	42.957133
3510.279513	1061076.719694	42.962138
3510.656586	1060869.458190	42.967143
3510.411907	1060660.654392	42.972148
3510.371398	1060455.179241	42.977153
3510.327460	1060239.200822	42.982157
3509.844921	1060043.123706	42.987162
3509.949306	1059830.378965	42.992167
3510.177825	1059641.489400	42.997172
3510.122351	1059428.273924	43.002177
3510.157156	1059219.562034	43.007181
3509.997524	1059033.990200	43.012186
3510.098181	1058814.464684	43.017191
3509.904468	1058605.959815	43.022196
3509.994859	1058405.588079	43.027201
3510.170670	1058204.328012	43.032205
3510.103580	1058012.637682	43.037210
3509.910986	1057810.942251	43.042215
3510.027578	1057613.716544	43.047220
3510.165958	1057412.915444	43.052225
3509.988461	1057203.391371	43.057229
3509.734972	1057011.215161	43.062234
3510.054146	1056803.039343	43.067239
3509.875207	1056614.016728	43.072244
3509.810585	1056407.141834	43.077249
3509.953442	1056213.619833	43.082253
3509.481866	1056026.456211	43.087258
3509.665304	1055813.639697	43.092263
3509.946311	1055623.061770	43.097268
3509.830459	1055437.554337	43.102273
3509.903480	1055235.046243	43.107277
3509.469352	1055028.758794	43.112282
3509.743918	1054834.202845	43.117287
3509.267684	1054651.812809	43.122292
3509.587757	1054458.296436	43.127297
3509.582067	1054257.307761	43.132301
3509.342126	1054063.580584	43.137306
3509.818359	1053879.080075	43.142311
3509.667548	1053685.710583	43.147316
3509.789117	1053486.504671	43.152321
3509.768279	1053282.301359	43.157325
3509.487117	1053104.263208	43.162330
3509.345817	1052899.101366	43.167335
3508.919127	1052710.660750	43.172340
3509.057222	1052538.417329	43.177345
3509.329993	1052349.849203	43.182349
3509.315728	1052166.433040	43.187354
3509.241781	1051968.458248	43.192359
3509.416827	1051784.708916	43.197364
3509.049353	1051610.880319	43.202369
3509.084674	1051416.436249	43.207373
3508.886010	1051237.359833	43.212378
3509.133366	1051053.284919	43.217383
3508.819514	1050877.688221	43.222388
3508.918960	1050688.127363	43.227393
3508.894413	1050508.516346	43.232397
3508.689882	1050333.752549	43.237402
3508.889483	1050157.276656	43.242407
3509.026997	1049970.868494	43.247412
3508.688028	1049794.083816	43.252417
3509.007519	1049609.948983	43.257421
3508.848956	1049451.551448	43.262426
3509.198119	1049273.478994	43.267431
3508.916421	1049085.469767	43.272436
3508.933238	1048908.598189	43.277441
3508.849179	1048714.175249	43.282445
3508.814438	1048541.835770	43.287450
3508.763870	1048349.324484	43.292455
3508.808251	1048176.478083	43.297460
3508.897690	1047997.828334	43.302465
3508.713103	1047821.630751	43.307469
3508.795396	1047656.096767	43.312474
3508.800912	1047481.304766	43.317479
3508.796050	1047292.802963	43.322484
3508.401933	1047119.127081	43.327489
3508.669486	1046931.919467	43.332493
3508.848743	1046769.914542	43.337498
3508.487927	1046588.301033	43.342503
3508.660084	1046407.945300	43.347508
3508.640585	1046233.118027	43.352513
3508.773451	1046061.928766	43.357517
3508.408546	1045892.071292	43.362522
3508.526065	1045716.336236	43.367527
3508.686043	1045543.967926	43.372532
3508.317828	1045372.260577	43.377537
3508.296593	1045194.504181	43.382541
3507.807907	1045041.152357	43.387546
3508.047166	1044872.612529	43.392551
3508.547351	1044705.762800	43.397556
3508.217776	1044532.091729	43.402561
3508.533124	1044372.215397	43.407565
3507.891271	1044214.809903	43.412570
3508.062632	1044042.199879	43.417575
3507.891124	1043894.269016	43.422580
3507.963367	1043722.051677	43.427585
3508.201730	1043556.176332	43.432589
3508.228945	1043400.182894	43.437594
3508.278188	1043228.147191	43.442599
3508.149532	1043064.346024	43.447604
3507.956437	1042900.067645	43.452609
3508.201699	1042733.876793	43.457613
3507.752331	1042570.017251	43.462618
3508.194936	1042406.682206	43.467623
3508.059365	1042246.818902	43.472628
3507.894665	1042087.921909	43.477633
3508.055424	1041925.488637	43.482637
3507.993716	1041782.893808	43.487642
3508.008305	1041596.320637	43.492647
3507.985480	1041438.637759	43.497652
3507.779525	1041271.607844	43.502657
3507.797952	1041121.735877	43.507661
3507.868833	1040969.242183	43.512666
3507.792813	1040803.529627	43.517671
3507.694697	1040655.596961	43.522676
3507.562620	1040498.291924	43.527681
3507.535965	1040341.834849	43.532685
3507.930712	1040174.479718	43.537690
3507.470472	1040016.635218	43.542695
3507.496295	1039872.237251	43.547700
3507.722054	1039707.795413	43.552705
3507.827965	1039565.019380	43.557709
3507.391036	1039412.083303	43.562714
3507.619276	1039248.787380	43.567719
3507.565649	1039095.586141	43.572724
3507.482711	1038944.608837	43.577729
3507.557657	1038788.574632	43.582733
3507.346225	1038647.180661	43.587738
3507.693081	1038495.153650	43.592743
3507.614578	1038335.168347	43.597748
3507.225766	1038188.474679	43.602753
3507.892152	1038033.385354	43.607757
3507.502350	1037884.266764	43.612762
3507.506367	1037729.084680	43.617767
3507.640414	1037574.747065	43.622772
3507.351156	1037428.307017	43.627777
3507.628090	1037269.392831	43.632781
3507.425285	1037119.836161	43.637786
3507.375711	1036959.516429	43.642791
3507.570799	1036812.110079	43.647796
3507.500023	1036666.581031	43.652801
3507.307607	1036523.195801	43.657805
3507.306206	1036374.262880	43.662810
3507.189067	1036210.354378	43.667815
3506.973158	1036076.729623	43.672820
3507.042813	1035937.541660	43.677825
3507.316193	1035785.646171	43.682829
3507.050083	1035645.345547	43.687834
3507.135454	1035498.696283	43.692839
3507.205219	1035356.398531	43.697844
3507.128148	1035220.408861	43.702849
3506.961550	1035062.762245	43.707853
3506.941510	1034930.625464	43.712858
3507.112732	1034787.329101	43.717863
3507.220006	1034638.235107	43.722868
3506.925604	1034496.652557	43.727873
3507.063869	1034360.122699	43.732877
3506.663775	1034222.033437	43.737882
3506.907586	1034069.805789	43.742887
3506.939683	1033931.928409	43.747892
3506.550596	1033809.210904	43.752897
3506.830668	1033660.255794	43.757901
3506.873314	1033527.978664	43.762906
3506.806826	1033382.169542	43.767911
3506.778698	1033250.187766	43.772916
3506.682373	1033117.536723	43.777921
3507.014500	1032973.102767	43.782925
3506.806411	1032850.527876	43.787930
3506.807285	1032714.173875	43.792935
3507.219700	1032574.651890	43.797940
3507.045468	1032433.481004	43.802945
3506.923140	1032278.748488	43.807949
3506.619752	1032143.592034	43.812954
3506.655767	1031996.181226	43.817959
3506.453992	1031870.583345	43.822964
3506.541497	1031742.611991	43.827969
3506.466024	1031609.437676	43.832973
3506.453290	1031477.024217	43.837978
3506.689077	1031339.242764	43.842983
3506.336057	1031216.171819	43.847988
3506.218997	1031085.508664	43.852993
3506.737538	1030961.126911	43.857997
3506.445049	1030842.490788	43.863002
3506.699022	1030697.429950	43.868007
3506.798278	1030563.427413	43.873012
3506.771622	1030424.311232	43.878017
3506.705449	1030285.875810	43.883021
3506.631161	1030157.120212	43.888026
3506.489227	1030021.304822	43.893031
3506.525685	1029885.650394	43.898036
3506.087033	1029764.788480	43.903041
3506.348259	1029620.182590	43.908045
3506.136664	1029512.736958	43.913050
3506.219396	1029375.319564	43.918055
3505.933887	1029257.229582	43.923060
3506.046425	1029131.227760	43.928065
3506.223676	1029007.246059	43.933069
3505.867410	1028888.772581	43.938074
3506.045232	1028765.560151	43.943079
3506.504154	1028640.264954	43.948084
3506.044274	1028526.062044	43.953089
3505.986353	1028386.900247	43.958093
3505.825530	1028267.606603	43.963098
3506.078754	1028151.147835	43.968103
3506.055407	1028033.182498	43.973108
3506.056142	1027919.278739	43.978113
3505.996793	1027786.204262	43.983117
3505.879416	1027670.087091	43.988122
3506.126746	1027542.283718	43.993127
3506.212792	1027427.968438	43.998132
3505.853507	1027319.633137	44.003137
3506.048793	1027181.077687	44.008141
3506.069032	1027069.672040	44.013146
3506.110778	1026953.804399	44.018151
3506.208671	1026822.521700	44.023156
3505.734101	1026708.671553	44.028161
3505.888808	1026582.217798	44.033165
3505.891482	1026462.761816	44.038170
3506.246239	1026337.335292	44.043175
3505.954413	1026232.746336	44.048180
3505.693968	1026116.911124	44.053185
3505.872294	1025997.513165	44.058189
3505.505658	1025872.195026	44.063194
3505.779332	1025758.105387	44.068199
3505.830369	1025654.321199	44.073204
3505.650640	1025530.321175	44.078209
3505.925543	1025402.270564	44.083213
3505.768537	1025295.510037	44.088218
3505.763842	1025178.062803	44.093223
3506.087692	1025064.144567	44.098228
3505.581163	1024948.034952	44.103233
3505.613545	1024821.173902	44.108237
3505.367542	1024724.011365	44.113242
3505.684139	1024604.076336	44.118247
3506.242425	1024491.076984	44.123252
3505.713711	1024377.188270	44.128257
3505.625867	1024260.801593	44.133261
3505.539296	1024146.738445	44.138266
3505.375019	1024032.685770	44.143271
3505.672035	1023927.375166	44.148276
3505.787516	1023822.092482	44.153281
3505.814486	1023701.798117	44.158285
3505.679874	1023590.542547	44.163290
3505.803366	1023471.487466	44.168295
3505.690211	1023373.504122	44.173300
3505.241648	1023252.309054	44.178305
3505.222904	1023131.622214	44.183309
3505.232337	1023030.704455	44.188314
3505.174600	1022930.183717	44.193319
3505.313236	1022830.695240	44.198324
3504.853709	1022722.190417	44.203329
3505.112176	1022609.881142	44.208333
3505.101774	1022524.954243	44.213338
3505.158993	1022417.037058	44.218343
3505.431884	1022312.960476	44.223348
3505.022028	1022201.140903	44.228353
3505.180051	1022103.672421	44.233357
3505.143736	1022000.125749	44.238362
3504.928841	1021890.497953	44.243367
3504.654221	1021797.458704	44.248372
3504.762872	1021701.542782	44.253377
3505.257323	1021602.846596	44.258381
3504.989399	1021504.565144	44.263386
3505.050105	1021418.834018	44.268391
3504.603573	1021313.208865	44.273396
3504.491627	1021217.320991	44.278401
3504.915218	1021118.724932	44.283405
3504.760461	1021027.204760	44.288410
3505.036655	1020932.508794	44.293415
3505.399249	1020822.668018	44.298420
3505.002056	1020735.159219	44.303425
3505.393571	1020635.784100	44.308429
3505.318406	1020530.276993	44.313434
3505.042388	1020421.697376	44.318439
3505.109415	1020319.848422	44.323444
3505.221841	1020224.100588	44.328449
3505.260172	1020106.539903	44.333453
3505.118855	1020018.201821	44.338458
3504.749011	1019912.149649	44.343463
3505.121978	1019813.732992	44.348468
3504.885496	1019725.696970	44.353473
3504.999715	1019603.360252	44.358477
3505.119904	1019505.658840	44.363482
3504.875071	1019408.694883	44.368487
3505.132312	1019302.818923	44.373492
3504.632304	1019215.109309	44.378497
3505.339309	1019113.521087	44.383501
3505.322711	1019023.594634	44.388506
3504.923572	1018918.110559	44.393511
3505.244386	1018809.110378	44.398516
3504.816692	1018724.000592	44.403521
3504.650787	1018612.748350	44.408525
3504.818900	1018522.880470	44.413530
3504.693934	1018442.470557	44.418535
3505.107041	1018334.901299	44.423540
3504.649153	1018255.319727	44.428545
3504.761305	1018151.483479	44.433549
3504.745291	1018054.458428	44.438554
3504.783164	1017955.579249	44.443559
3505.067702	1017855.105190	44.448564
3504.577853	1017763.781015	44.453569
3504.488265	1017664.432533	44.458573
3504.611483	1017582.416857	44.463578
3504.573079	1017498.388800	44.468583
3504.465032	1017410.004168	44.473588
3504.228579	1017321.930416	44.478593
3504.791285	1017220.525823	44.483597
3504.650461	1017127.192941	44.488602
3504.483730	1017039.103270	44.493607
3504.853986	1016946.750722	44.498612
3504.618288	1016867.015814	44.503617
3504.352797	1016771.271319	44.508621
3504.500851	1016677.786339	44.513626
3504.428334	1016588.218292	44.518631
3504.395424	1016504.368567	44.523636
3504.363653	1016425.661414	44.528641
3504.276693	1016335.412318	44.533645
3504.263175	1016249.323249	44.538650
3504.210177	1016159.939279	44.543655
3504.494774	1016074.089612	44.548660
3504.223086	1016001.142731	44.553665
3504.413036	1015903.367147	44.558669
3504.345574	1015825.433991	44.563674
3504.351450	1015730.888939	44.568679
3504.675099	1015635.901678	44.573684
3504.346985	1015574.218705	44.578689
3504.149813	1015485.818472	44.583693
3504.230013	1015400.962922	44.588698
3504.291624	1015318.438975	44.593703
3504.524910	1015240.351098	44.598708
3503.972026	1015149.383072	44.603713
3504.339774	1015063.115961	44.608717
3504.474608	1014981.157486	44.613722
3503.746580	1014901.475760	44.618727
3504.466420	1014814.758519	44.623732
3503.801155	1014724.675885	44.628737
3504.381089	1014654.386753	44.633741
3504.260219	1014589.357860	44.638746
3504.027104	1014492.307038	44.643751
3504.169539	1014403.736762	44.648756
3504.088873	1014340.251832	44.653761
3504.000186	1014262.106311	44.658765
3503.826365	1014173.972881	44.663770
3503.753954	1014102.230767	44.668775
3504.070237	1014026.248498	44.673780
3504.166172	1013961.370830	44.678785
3504.026240	1013863.419911	44.683789
3503.955196	1013788.954747	44.688794
3503.987367	1013720.297810	44.693799
3504.175902	1013639.379080	44.698804
3503.728716	1013570.410844	44.703809
3504.129894	1013484.502452	44.708813
3504.022749	1013411.106416	44.713818
3503.941433	1013333.238101	44.718823
3504.190431	1013258.810319	44.723828
3503.852896	1013176.417793	44.728833
3503.852028	1013104.845401	44.733837
3504.299478	1013020.767482	44.738842
3503.894333	1012930.613240	44.743847
3503.952986	1012863.689597	44.748852
3503.941980	1012799.301737	44.753857
3503.804090	1012713.955972	44.758861
3503.951520	1012627.299329	44.763866
3503.837264	1012561.080424	44.768871
3503.948646	1012496.668944	44.773876
3503.891911	1012420.143689	44.778881
3504.007435	1012335.721710	44.783885
3503.915260	1012265.804852	44.788890
3503.928201	1012182.465885	44.793895
3504.250622	1012102.085788	44.798900
3504.107321	1012029.843265	44.803905
3503.878591	1011934.981640	44.808909
3504.327862	1011863.513595	44.813914
3504.035873	1011779.150390	44.818919
3504.465325	1011703.700966	44.823924
3503.915339	1011623.069166	44.828929
3504.097772	1011550.086861	44.833933
3504.036266	1011482.098036	44.838938
3504.104324	1011396.018373	44.843943
3504.242195	1011311.091636	44.848948
3504.195183	1011230.954248	44.853953
3504.094183	1011156.750625	44.858957
3504.070302	1011088.653706	44.863962
3503.747972	1011010.695803	44.868967
3503.968876	1010921.280602	44.873972
3503.909438	1010848.523348	44.878977
3504.121028	1010773.874585	44.883981
3503.967937	1010697.827562	44.888986
3503.486350	1010628.343127	44.893991
3504.111828	1010554.109070	44.898996
3503.904396	1010485.840778	44.904001
3504.002130	1010404.501880	44.909005
3503.927499	1010327.951137	44.914010
3503.579241	1010251.347257	44.919015
3503.916588	1010166.661908	44.924020
3503.891439	1010118.472217	44.929025
3503.883126	1010036.270980	44.934029
3503.833556	1009966.221383	44.939034
3503.724071	1009899.970390	44.944039
3503.759238	1009815.329534	44.949044
3503.353780	1009754.761487	44.954049
3504.027834	1009677.884260	44.959053
3503.568275	1009611.979058	44.964058
3503.425511	1009542.522589	44.969063
3503.697158	1009474.649014	44.974068
3503.543055	1009407.330634	44.979073
3503.411849	1009335.731799	44.984077
3503.769546	1009273.186477	44.989082
3503.604225	1009199.647927	44.994087
3503.807340	1009127.699843	44.999092
3503.488131	1009058.752386	45.004097
3503.643964	1008977.674881	45.009101
3503.975634	1008922.516037	45.014106
3503.795546	1008847.809095	45.019111
3503.978090	1008778.581196	45.024116
3503.646616	1008715.462878	45.029121
3503.747050	1008631.668210	45.034125
3503.699441	1008562.572757	45.039130
3503.725260	1008493.075590	45.044135
3503.803151	1008421.527898	45.049140
3503.525006	1008356.744465	45.054145
3503.824544	1008270.481739	45.059149
3503.877926	1008218.083374	45.064154
3503.148953	1008136.264717	45.069159
3503.814811	1008065.587671	45.074164
3503.584935	1007997.973335	45.079169
3503.580081	1007930.807143	45.084173
3503.875039	1007864.562817	45.089178
3503.700999	1007792.465413	45.094183
3503.890895	1007720.598768	45.099188
3503.887600	1007650.415566	45.104193
3503.619209	1007577.067241	45.109197
3503.497184	1007521.969436	45.114202
3503.270896	1007443.363075	45.119207
3503.595218	1007385.274068	45.124212
3503.379606	1007315.996588	45.129217
3503.715387	1007260.820831	45.134221
3503.568152	1007183.753270	45.139226
3503.611576	1007121.916386	45.144231
3503.444940	1007041.544690	45.149236
3503.451475	1006979.031785	45.154241
3503.452222	1006912.533086	45.159245
3503.545235	1006840.962861	45.164250
3503.286862	1006784.810868	45.169255
3503.456331	1006710.212477	45.174260
3503.388657	1006661.708569	45.179265
3503.577803	1006603.731014	45.184269
3503.604718	1006534.209536	45.189274
3503.333853	1006456.763497	45.194279
3503.925680	1006403.092852	45.199284
3503.560497	1006341.023022	45.204289
3503.445134	1006264.715504	45.209293
3503.518585	1006198.585348	45.214298
3503.510775	1006136.551641	45.219303
3503.594746	1006067.890132	45.224308
3503.758304	1006000.284282	45.229313
3503.621745	1005923.392222	45.234317
3503.223409	1005864.142502	45.239322
3503.032907	1005797.370448	45.244327
3503.585537	1005728.530384	45.249332
3503.349240	1005673.919558	45.254337
3502.930728	1005611.558756	45.259341
3503.233406	1005556.177318	45.264346
3502.918656	1005498.465898	45.269351
3503.145658	1005435.121622	45.274356
3503.216777	1005390.182042	45.279361
3503.410707	1005337.053050	45.284365
3503.244472	1005266.867043	45.289370
3503.257339	1005196.067162	45.294375
3503.508622	1005135.827547	45.299380
3503.285083	1005073.331433	45.304385
3503.089244	1005008.106962	45.309389
3503.205160	1004949.249204	45.314394
3503.129427	1004889.741608	45.319399
3503.443878	1004824.041944	45.324404
3503.185264	1004764.660408	45.329409
3503.097015	1004701.554349	45.334413
3503.478140	1004650.916809	45.339418
3503.261433	1004581.994979	45.344423
3503.435609	1004512.035307	45.349428
3502.854448	1004460.679192	45.354433
3503.148025	1004405.677035	45.359437
3503.104635	1004354.717705	45.364442
3503.092101	1004294.609840	45.369447
3503.277381	1004222.213103	45.374452
3503.538910	1004171.299166	45.379457
3503.021741	1004114.871421	45.384461
3503.179610	1004042.476897	45.389466
3503.204726	1003987.125803	45.394471
3503.198291	1003928.569381	45.399476
3502.984694	1003874.229221	45.404481
3502.649873	1003814.558423	45.409485
3503.021143	1003764.790042	45.414490
3502.811020	1003706.167588	45.419495
3503.047578	1003655.155841	45.424500
3503.113710	1003604.366259	45.429505
3503.042028	1003549.513212	45.434509
3503.215870	1003499.677738	45.439514
3503.050895	1003439.683167	45.444519
3503.147163	1003366.122760	45.449524
3502.693905	1003327.965594	45.454529
3502.758593	1003277.076027	45.459533
3503.277169	1003210.448446	45.464538
3503.272070	1003162.293310	45.469543
3503.466288	1003092.701915	45.474548
3503.007368	1003029.443656	45.479553
3503.213812	1002976.971438	45.484557
3503.216323	1002923.170268	45.489562
3503.032780	1002861.226823	45.494567
3503.097538	1002791.263880	45.499572
3502.731750	1002734.700111	45.504577
3502.895469	1002695.950591	45.509581
3502.997386	1002651.762511	45.514586
3502.733972	1002591.483266	45.519591
3503.007854	1002536.563474	45.524596
3503.032512	1002494.332812	45.529601
3503.128446	1002437.300833	45.534605
3502.938619	1002374.088211	45.539610
3502.668226	1002331.904932	45.544615
3502.997071	1002270.551721	45.549620
3502.873651	1002221.824257	45.554625
3502.596867	1002167.088877	45.559629
3502.888341	1002119.849042	45.564634
3502.666514	1002065.882057	45.569639
3502.977437	1002010.756454	45.574644
3502.643548	1001968.970144	45.579649
3502.585305	1001914.682855	45.584653
3502.937015	1001870.350224	45.589658
3502.223642	1001820.840701	45.594663
3502.820790	1001765.957499	45.599668
3502.541307	1001722.506144	45.604673
3502.639136	1001683.857856	45.609677
3502.788097	1001633.134240	45.614682
3502.509612	1001590.460200	45.619687
3502.783451	1001538.547418	45.624692
3502.604083	1001496.440224	45.629697
3502.743532	1001442.797045	45.634701
3502.951074	1001392.256252	45.639706
3502.508020	1001354.667960	45.644711
3503.028974	1001298.819619	45.649716
3502.851585	1001247.173119	45.654721
3502.987776	1001193.236158	45.659725
3503.014963	1001146.518328	45.664730
3502.850860	1001076.377229	45.669735
3503.069764	1001031.184013	45.674740
3502.600278	1000986.882397	45.679745
3502.641274	1000926.437937	45.684749
3502.872514	1000875.304684	45.689754
3502.837976	1000833.168696	45.694759
3502.884636	1000774.278886	45.699764
3502.861392	1000724.840739	45.704769
3502.715077	1000679.412886	45.709773
3503.192422	1000641.570930	45.714778
3502.729463	1000586.072274	45.719783
3502.851131	1000519.478404	45.724788
3502.877323	1000475.577796	45.729793
3502.567749	1000429.980165	45.734797
3502.720802	1000384.500637	45.739802
3502.648557	1000337.695174	45.744807
3502.984000	1000276.805946	45.749812
3503.157481	1000212.146629	45.754817
3502.851919	1000149.025533	45.759821
3502.771681	1000037.489253	45.764826
3502.492835	999863.587497	45.769831
3502.455301	999635.029752	45.774836
3502.511719	999357.966785	45.779841
3502.346873	999008.396301	45.784845
3502.578557	998589.708228	45.789850
3502.287285	998117.131414	45.794855
3501.924936	997575.678591	45.799860
3502.322829	996983.307988	45.804865
3502.099406	996296.107653	45.809869
3501.771422	995556.431602	45.814874
3502.128573	994762.570402	45.819879
3501.994176	993880.979369	45.824884
3501.406672	992934.514755	45.829889
3501.303006	991917.433578	45.834893
3501.496845	990823.001443	45.839898
3501.231464	989664.463318	45.844903
3500.777498	988412.376497	45.849908
3500.498146	987098.131955	45.854913
3500.348218	985702.567703	45.859917
3500.538559	984236.131477	45.864922
3499.860848	982704.142716	45.869927
3499.691858	981046.160928	45.874932
3499.467461	979336.124659	45.879937
3499.230329	977545.347435	45.884941
3499.202822	975662.573124	45.889946
3498.702539	973705.230746	45.894951
3498.416083	971659.338174	45.899956
3497.948701	969535.142022	45.904961
3497.635241	967315.075161	45.909965
3497.414173	965013.238830	45.914970
3497.162874	962656.206535	45.919975
3496.986681	960200.765823	45.924980
3496.281307	957665.720181	45.929985
3496.148687	955039.698625	45.934989
3495.722866	952396.974579	45.939994
3495.006804	949682.408395	45.944999
3494.853886	946877.347823	45.950004
3494.212724	944004.919663	45.955009
3493.546841	941040.209466	45.960013
3493.269626	937990.100693	45.965018
3492.560722	934879.163197	45.970023
3492.081329	931672.904402	45.975028
3491.380217	928398.916534	45.980033
3490.896569	925039.033706	45.985037
3490.522229	921603.808283	45.990042
3489.675635	918093.111888	45.995047
3489.557179	914494.862597	46.000052
3488.732025	910809.624459	46.005057
3487.814204	907047.174885	46.010061
3487.455357	903200.125610	46.015066
3486.500503	899294.889732	46.020071
3486.122026	895283.898723	46.025076
3485.341142	891203.492579	46.030081
3484.485726	887048.169266	46.035085
3483.915704	882793.899566	46.040090
3483.152293	878482.364802	46.045095
3482.343407	874066.285818	46.050100
3481.816265	869582.598543	46.055105
3480.884589	865018.760761	46.060109
3480.298122	860363.706281	46.065114
3479.244358	855627.226609	46.070119
3478.328518	850811.312202	46.075124
3477.253259	845927.272397	46.080129
3476.760132	840940.722266	46.085133
3476.115326	835883.462293	46.090138
3474.812501	830738.451807	46.095143
3474.083758	825524.345911	46.100148
3473.201732	820217.170914	46.105153
3472.223480	814822.964473	46.110157
3471.651285	809355.406756	46.115162
3470.255305	803810.261721	46.120167
3469.250780	798163.584563	46.125172
3468.359733	792441.519617	46.130177
3466.852764	786646.573052	46.135181
3466.243100	780759.877686	46.140186
3465.029175	774794.427741	46.145191
3463.858031	768742.795942	46.150196
3462.746212	762622.057522	46.155201
3461.633493	756405.860556	46.160205
3460.846197	750110.350404	46.165210
3459.142293	743731.611469	46.170215
3458.240256	737274.238104	46.175220
3457.322579	730726.766505	46.180225
3455.976615	724099.395137	46.185229
3454.666412	717392.936449	46.190234
3453.361967	710585.896853	46.195239
3452.275429	703687.686700	46.200244
3450.658368	696736.903288	46.205249
3449.443432	689691.809874	46.210253
3448.299706	682566.838079	46.215258
3446.750003	675370.162173	46.220263
3445.494526	668066.289588	46.225268
3443.983231	660701.309113	46.230273
3442.666974	653244.545429	46.235277
3441.147799	645729.826860	46.240282
3439.708745	638119.820870	46.245287
3438.214991	630422.576391	46.250292
3436.607793	622672.266958	46.255297
3435.211876	614823.523495	46.260301
3433.841498	606891.356491	46.265306
3431.980792	598889.573610	46.270311
3430.675651	590794.281531	46.275316
3428.897016	582649.302255	46.280321
3426.998680	574412.862100	46.285325
3424.951435	566100.193654	46.290330
3423.568379	557719.332812	46.295335
3421.407871	549249.776082	46.300340
3419.713982	540717.597474	46.305345
3418.030483	532115.252003	46.310349
3416.400087	523433.181258	46.315354
3414.394047	514672.905282	46.320359
3412.696367	505847.248426	46.325364
3410.761840	496950.150769	46.330369
3408.500390	487975.875901	46.335373
3406.928023	478919.918592	46.340378
3404.189255	469809.454301	46.345383
3402.632277	460627.687648	46.350388
3400.638535	451389.081282	46.355393
3398.096037	442067.347833	46.360397
3396.670672	432677.130942	46.365402
3394.350391	423220.715399	46.370407
3391.899337	413704.002467	46.375412
3389.702875	404107.745865	46.380417
3387.474992	394454.950692	46.385421
3385.266459	384733.931515	46.390426
3382.295541	374965.833209	46.395431
3380.161288	365128.557277	46.400436
3377.889231	355238.777952	46.405441
3374.853841	345308.758786	46.410445
3372.305529	335300.103505	46.415450
3369.764474	325264.460408	46.420455
3367.009046	315162.359091	46.425460
3364.225610	305006.214151	46.430465
3361.530317	294814.679551	46.435469
3358.434509	284571.174790	46.440474
3355.564415	274286.315396	46.445479
3352.305994	263945.461802	46.450484
3349.484225	253577.752839	46.455489
3346.132944	243185.836027	46.460493
3343.260776	232744.075641	46.465498
3339.911748	222183.603771	46.470503
3336.455980	211668.353082	46.475508
3333.077239	201129.764296	46.480513
3329.452351	190563.173021	46.485517
3326.137671	179994.990054	46.490522
3322.286284	169383.602260	46.495527
3318.248621	158750.895769	46.500532
3314.369052	148125.060334	46.505537
3310.056999	137490.379940	46.510541
3305.991680	126846.528195	46.515546
3301.390425	116205.743072	46.520551
3296.639001	105564.880995	46.525556
3291.817780	94960.001297	46.530561
3286.772646	84351.556795	46.535565
3281.401224	73762.681174	46.540570
3275.362646	63234.201540	46.545575
3269.156968	52737.330076	46.550580
3261.594026	42318.435378	46.555585
3246.883191	32183.712054	46.560589
3216.170126	22627.836239	46.565594
3177.749511	13609.721114	46.570599
3122.247024	5625.963613	46.575604
2990.119756	592.616330	46.580609
2741.561394	400.836229	46.585613
2604.885822	375.002529	46.590618
2589.887384	354.263347	46.595623
2656.313528	340.129866	46.600628
2751.097783	347.561429	46.605633
2832.795199	351.914905	46.610637
2884.163679	331.833256	46.615642
2903.488774	336.008153	46.620647
2901.386119	327.851313	46.625652
2888.468962	321.104904	46.630657
2873.955696	327.782468	46.635661
2862.718192	328.380468	46.640666
2855.781099	329.947427	46.645671
2852.724601	338.479347	46.650676
2851.698494	320.336931	46.655681
2850.634177	307.148347	46.660685
2849.499325	315.894641	46.665690
2847.468953	333.429070	46.670695
2844.936114	328.492837	46.675700
2842.325069	324.188088	46.680705
2839.008377	315.890060	46.685709
2835.939778	305.966392	46.690714
2832.708490	313.950266	46.695719
2829.438448	322.105194	46.700724
2826.385843	308.804581	46.705729
2823.241579	311.521055	46.710733
2820.692735	302.410093	46.715738
2816.964849	297.685595	46.720743
2813.700411	303.112389	46.725748
2810.902396	305.056314	46.730753
2807.286769	302.005301	46.735757
2804.181329	288.101255	46.740762
2801.094108	303.338404	46.745767
2797.361599	293.689271	46.750772
2794.183792	295.010929	46.755777
2790.697279	300.420869	46.760781
2787.942372	290.812627	46.765786
2784.223671	294.077050	46.770791
2780.826302	291.172291	46.775796
2777.788879	281.366950	46.780801
2774.288770	282.499547	46.785805
2771.462837	292.055311	46.790810
2768.050649	288.242782	46.795815
2764.460282	284.505114	46.800820
2761.008461	279.889242	46.805825
2757.914155	275.413621	46.810829
2754.548306	287.145608	46.815834
2750.712670	284.310062	46.820839
2747.457075	289.564739	46.825844
2744.299074	281.932504	46.830849
2740.337522	287.083960	46.835853
2737.120992	273.022373	46.840858
2733.625788	281.804902	46.845863
2730.396987	280.826791	46.850868
2727.130367	280.096629	46.855873
2723.848154	280.029258	46.860877
2720.265543	275.531853	46.865882
2716.559318	272.912264	46.870887
2713.087816	270.207411	46.875892
2709.866149	279.717833	46.880897
2706.270591	276.082275	46.885901
2703.538144	278.587837	46.890906
2700.012681	267.602160	46.895911
2696.306440	267.709487	46.900916
2693.094646	267.395121	46.905921
2689.009961	285.445105	46.910925
2685.434031	271.812278	46.915930
2681.874836	275.764530	46.920935
2678.763562	267.937970	46.925940
2676.048108	265.250253	46.930945
2672.236964	270.037355	46.935949
2668.323039	273.269788	46.940954
2665.178609	267.983517	46.945959
2662.039878	268.744129	46.950964
2658.089414	266.644909	46.955969
2654.363787	267.661722	46.960973
2651.233364	266.487375	46.965978
2647.866899	271.273585	46.970983
2644.322323	264.842770	46.975988
2641.535719	264.916783	46.980993
2638.009154	273.233225	46.985997
2634.028986	256.215059	46.991002
2630.126069	271.208259	46.996007
2626.817109	261.134243	47.001012
2624.069559	256.768048	47.006017
2620.579919	265.268320	47.011021
2616.716764	257.741675	47.016026
2613.143585	256.592204	47.021031
2609.826842	258.758266	47.026036
2606.881412	256.107115	47.031041
2602.476422	264.748652	47.036045
2599.118012	262.200227	47.041050
2595.969730	253.770803	47.046055
2592.045118	256.257798	47.051060
2588.691233	256.376335	47.056065
2585.632274	254.143180	47.061069
2582.208489	250.293299	47.066074
2578.651870	245.873675	47.071079
2575.178412	243.925228	47.076084
2571.900517	238.100940	47.081089
2567.880087	254.989002	47.086093
2564.413790	243.946210	47.091098
2561.355990	246.547983	47.096103
2557.628275	241.425037	47.101108
2554.298097	251.625539	47.106113
2550.354799	248.614884	47.111117
2547.310925	248.944947	47.116122
2543.561338	255.892122	47.121127
2540.037400	249.182218	47.126132
2536.907134	246.072235	47.131137
2533.347798	246.239867	47.136141
2529.997855	243.977569	47.141146
2526.459245	245.692682	47.146151
2522.704976	252.247980	47.151156
2519.122269	234.724366	47.156161
2515.409115	249.327378	47.161165
2512.655317	242.514275	47.166170
2508.889291	244.355293	47.171175
2505.502983	242.234657	47.176180
2501.696517	240.468328	47.181185
2498.070114	243.791643	47.186189
2494.968338	234.064469	47.191194
2491.511485	243.557585	47.196199
2488.050092	243.246582	47.201204
2484.414927	231.303325	47.206209
2480.850791	250.446357	47.211213
2477.839559	225.861749	47.216218
2474.124676	234.657881	47.221223
2470.773360	236.870246	47.226228
2467.233337	233.966776	47.231233
2463.735537	241.103711	47.236237
2460.087130	233.641401	47.241242
2456.689658	228.602473	47.246247
2452.810959	228.845301	47.251252
2449.564455	233.035735	47.256257
2446.157309	246.263830	47.261261
2442.215477	234.789869	47.266266
2439.155436	232.905120	47.271271
2435.603371	241.931324	47.276276
2432.329025	222.955404	47.281281
2428.853002	231.294644	47.286285
2425.175634	231.456634	47.291290
2421.638771	226.515591	47.296295
2418.060885	230.353427	47.301300
2414.627907	232.936027	47.306305
2410.919718	230.951884	47.311309
2407.808019	224.814069	47.316314
2404.349490	223.694136	47.321319
2400.517340	224.059148	47.326324
2397.342552	220.679644	47.331329
2393.435077	227.150545	47.336333
2390.359512	227.866121	47.341338
2386.885262	219.535270	47.346343
2383.401351	226.507056	47.351348
2380.106932	220.442601	47.356353
2376.287985	229.495469	47.361357
2372.772865	232.689891	47.366362
2369.461136	234.745712	47.371367
2365.638702	224.620494	47.376372
2362.272696	229.720852	47.381377
2358.559207	225.741676	47.386381
2355.592905	217.934309	47.391386
2351.864129	228.081124	47.396391
2347.974713	225.623848	47.401396
2344.633534	216.992370	47.406401
2341.067184	216.086577	47.411405
2337.748620	218.650535	47.416410
2334.342929	220.325955	47.421415
2330.448817	230.146853	47.426420
2327.665351	214.622475	47.431425
2323.947401	223.861544	47.436429
2320.658404	216.986054	47.441434
2317.306406	220.622216	47.446439
2313.223722	221.675386	47.451444
2309.956407	225.071069	47.456449
2306.059997	219.458535	47.461453
2302.633862	210.787917	47.466458
2299.235207	216.287815	47.471463
2295.696475	216.782366	47.476468
2292.504529	209.361198	47.481473
2288.911933	220.729046	47.486477
2285.342376	214.783419	47.491482
2281.947427	221.455648	47.496487
2278.399033	215.544616	47.501492
2275.227243	210.172396	47.506497
2271.250375	219.873183	47.511501
2267.659105	222.722378	47.516506
2264.300954	217.597844	47.521511
2260.809625	224.581456	47.526516
2257.622332	211.736161	47.531521
2253.553806	219.607877	47.536525
2250.651990	213.669245	47.541530
2247.006179	215.641010	47.546535
2243.411952	217.599239	47.551540
2239.977340	215.894547	47.556545
2236.404928	211.798251	47.561549
2232.904272	211.113619	47.566554
2229.365496	220.933760	47.571559
2225.753178	211.150753	47.576564
2222.341932	205.372816	47.581569
2218.678360	206.192252	47.586573
2215.409342	204.134101	47.591578
2212.062608	201.015581	47.596583
2208.461540	213.705175	47.601588
2205.264371	211.427209	47.606593
2201.363166	215.318660	47.611597
2197.651282	211.048667	47.616602
2194.331043	217.716005	47.621607
2190.903415	213.104146	47.626612
2187.734306	212.627671	47.631617
2183.646980	204.986945	47.636621
2180.658716	215.948129	47.641626
2177.367340	206.446763	47.646631
2173.660928	207.717045	47.651636
2170.158074	209.953542	47.656641
2166.467268	210.290129	47.661645
2162.597762	206.701237	47.666650
2159.531035	214.545578	47.671655
2155.927328	203.711784	47.676660
2152.054001	211.340221	47.681665
2148.525563	209.503459	47.686669
2145.698676	198.330220	47.691674
2142.190413	203.648772	47.696679
2138.439553	208.514255	47.701684
2134.987890	209.509015	47.706689
2131.351861	209.693038	47.711693
2128.512109	203.682863	47.716698
2124.818433	196.588228	47.721703
2120.759439	208.699486	47.726708
2117.028055	196.315178	47.731713
2113.211879	202.053309	47.736717
2110.369072	202.668254	47.741722
2107.198780	205.324067	47.746727
2103.274195	219.907706	47.751732
2100.251663	207.237573	47.756737
2096.358201	205.056754	47.761741
2093.005842	198.805881	47.766746
2089.822682	199.484374	47.771751
2086.127554	206.669282	47.776756
2082.716196	206.983394	47.781761
2078.735940	200.378828	47.786765
2075.133863	197.609515	47.791770
2071.786467	207.790791	47.796775
2068.434205	206.551380	47.801780
2064.943548	201.180168	47.806785
2061.476475	214.764132	47.811789
2058.040226	211.744999	47.816794
2054.763807	200.572656	47.821799
2050.850062	209.295395	47.826804
2047.509947	208.619885	47.831809
2043.879514	211.357745	47.836813
2040.358845	211.724833	47.841818
2037.112090	200.432868	47.846823
2033.411010	199.336551	47.851828
2030.115466	201.707417	47.856833
2026.356085	206.723427	47.861837
2022.796881	200.809291	47.866842
2019.335743	199.309456	47.871847
2015.608746	195.528240	47.876852
2012.522687	202.361327	47.881857
2008.866288	209.216583	47.886861
2005.390053	204.868657	47.891866
2001.810001	196.104428	47.896871
1998.570109	205.752217	47.901876
1995.524620	189.823466	47.906881
1991.442738	208.938732	47.911885
1987.788584	201.458714	47.916890
1984.667025	205.988610	47.921895
1980.845992	199.504342	47.926900
1977.421487	196.915235	47.931905
1973.557174	200.336923	47.936909
1970.248289	205.897414	47.941914
1967.169477	190.441710	47.946919
1963.303301	190.907663	47.951924
1959.817474	185.494478	47.956929
1956.203803	197.074663	47.961933
1952.768654	197.278516	47.966938
1949.777585	189.873722	47.971943
1946.093485	198.985898	47.976948
1942.668051	193.321244	47.981953
1939.164041	198.105643	47.986957
1935.176982	193.497028	47.991962
1931.953814	183.806287	47.996967
1928.547283	195.437350	48.001972
1924.944101	184.652064	48.006977
1921.315436	201.028260	48.011981
1917.850268	191.734484	48.016986
1914.622187	194.311116	48.021991
1911.024446	197.147133	48.026996
1907.488359	180.793470	48.032001
1903.530755	193.314967	48.037005
1900.047831	189.411172	48.042010
1896.991258	188.050648	48.047015
1893.510868	197.986957	48.052020
1890.118068	195.052790	48.057025
1886.179029	187.440580	48.062029
1882.877218	192.118636	48.067034
1879.853352	188.694454	48.072039
1875.921308	190.042752	48.077044
1872.382742	180.506783	48.082049
1868.770942	189.388533	48.087053
1865.465375	192.834997	48.092058
1862.297015	186.428798	48.097063
1858.289570	197.064237	48.102068
1855.044105	181.265057	48.107073
1850.987300	189.922588	48.112077
1847.636978	190.151365	48.117082
1844.485263	191.947683	48.122087
1840.809340	192.468438	48.127092
1837.416227	189.194578	48.132097
1833.772548	187.801509	48.137101
1830.720362	195.246558	48.142106
1827.053368	185.117271	48.147111
1822.993266	195.985165	48.152116
1819.982827	177.721865	48.157121
1816.255032	187.533075	48.162125
1812.997777	187.571990	48.167130
1809.265857	187.955298	48.172135
1805.663963	187.674014	48.177140
1802.455479	172.985564	48.182145
1798.811858	183.101452	48.187149
1795.440526	178.686219	48.192154
1791.770910	185.012277	48.197159
1788.255726	194.614196	48.202164
1784.936312	177.771937	48.207169
1781.166799	178.744126	48.212173
1777.597484	188.225540	48.217178
1774.632163	184.507814	48.222183
1770.975841	186.176591	48.227188
1767.836549	176.050647	48.232193
1763.991919	193.839465	48.237197
1760.102488	180.863888	48.242202
1756.728914	180.376551	48.247207
1752.857039	180.635095	48.252212
1749.735014	176.274744	48.257217
1746.363283	177.520892	48.262221
1742.884059	173.198863	48.267226
1739.626414	176.402373	48.272231
1735.810879	189.517688	48.277236
1732.076277	176.340782	48.282241
1728.680375	173.025808	48.287245
1725.216113	178.004896	48.292250
1721.794684	179.280861	48.297255
1718.098145	178.082345	48.302260
1715.165715	174.247149	48.307265
1711.789665	175.254883	48.312269
1707.742485	178.356643	48.317274
1704.578768	177.591417	48.322279
1700.874533	182.161918	48.327284
1697.147033	168.127436	48.332289
1693.421896	180.331356	48.337293
1690.349588	174.783987	48.342298
1686.780470	168.404551	48.347303
1683.341949	188.463148	48.352308
1680.103256	177.999674	48.357313
1676.305170	181.438004	48.362317
1672.707371	182.049444	48.367322
1669.631640	175.668216	48.372327
1665.341909	186.999965	48.377332
1662.131244	181.408845	48.382337
1658.606177	179.105333	48.387341
1655.369924	176.634199	48.392346
1652.050358	176.435251	48.397351
1648.189848	182.663434	48.402356
1644.530419	179.874219	48.407361
1640.936758	174.495973	48.412365
1637.429852	183.559494	48.417370
1634.575141	176.277486	48.422375
1631.136775	185.317369	48.427380
1627.416781	175.147432	48.432385
1623.718531	179.204561	48.437389
1620.124266	183.066557	48.442394
1616.599698	174.699877	48.447399
1612.906071	167.242888	48.452404
1609.658766	168.444198	48.457409
1605.958054	173.993222	48.462413
1602.702835	174.747549	48.467418
1599.606264	176.096736	48.472423
1595.526049	187.112577	48.477428
1592.240048	179.248853	48.482433
1588.790455	170.446091	48.487437
1585.102107	181.738419	48.492442
1582.024915	174.120922	48.497447
1578.156106	173.929380	48.502452
1574.866269	165.817889	48.507457
1571.154587	176.252508	48.512461
1567.859427	170.631581	48.517466
1563.959386	175.992825	48.522471
1560.641534	182.630599	48.527476
1557.219297	177.685821	48.532481
1553.423921	170.523473	48.537485
1550.160389	180.979350	48.542490
1547.226700	174.978937	48.547495
1543.335266	188.695236	48.552500
1539.788525	170.932412	48.557505
1536.094296	181.323719	48.562509
1532.274197	179.569048	48.567514
1528.866518	182.889060	48.572519
1525.558582	178.392473	48.577524
1522.348395	170.424135	48.582529
1518.550069	171.395099	48.587533
1515.174531	174.261320	48.592538
1511.421965	169.057950	48.597543
1507.912140	171.233744	48.602548
1504.940673	163.539947	48.607553
1500.991498	172.782363	48.612557
1497.810615	171.261697	48.617562
1494.680852	171.342166	48.622567
1490.721574	180.750620	48.627572
1487.079576	174.663703	48.632577
1483.503637	177.795347	48.637581
1480.110224	176.282830	48.642586
1476.457793	181.167097	48.647591
1472.857953	177.822377	48.652596
1469.406585	174.135089	48.657601
1466.007830	183.715644	48.662605
1462.462233	179.994384	48.667610
1459.487278	171.338003	48.672615
1455.666959	180.740509	48.677620
1452.089559	170.459053	48.682625
1448.280210	166.537754	48.687629
1444.867290	172.850503	48.692634
1441.909163	163.114333	48.697639
1438.197894	171.706538	48.702644
1434.652679	175.364198	48.707649
1431.071323	166.589000	48.712653
1426.970716	173.823049	48.717658
1424.299028	179.433278	48.722663
1420.446019	171.186726	48.727668
1417.276945	175.914687	48.732673
1413.513499	171.810321	48.737677
1410.040476	173.878572	48.742682
1406.697406	171.867661	48.747687
1403.068356	167.214496	48.752692
1399.480171	162.523021	48.757697
1396.244793	175.277716	48.762701
1392.674042	167.903972	48.767706
1389.118804	162.877060	48.772711
1385.492176	165.081760	48.777716
1382.143028	159.391711	48.782721
1378.705156	167.688823	48.787725
1374.719963	176.565312	48.792730
1371.250495	163.697890	48.797735
1367.897800	167.366720	48.802740
1364.768195	170.728611	48.807745
1361.192271	176.606691	48.812749
1357.750817	159.272554	48.817754
1354.081489	167.673188	48.822759
1350.524038	166.064197	48.827764
1346.949297	158.333812	48.832769
1343.501465	171.496703	48.837773
1339.713596	182.116348	48.842778
1336.620027	163.879122	48.847783
1333.294006	178.491099	48.852788
1329.771871	172.404518	48.857793
1325.707756	167.533949	48.862797
1322.131364	165.629173	48.867802
1318.898597	164.116267	48.872807
1315.504141	169.546803	48.877812
1312.075473	161.830111	48.882817
1308.489949	170.144027	48.887821
1305.007121	174.460534	48.892826
1301.752488	167.522616	48.897831
1298.098020	174.138216	48.902836
1294.269188	167.932494	48.907841
1290.851121	169.572444	48.912845
1287.305601	169.211977	48.917850
1283.846343	164.446603	48.922855
1280.439673	170.861583	48.927860
1277.093178	167.208588	48.932865
1273.795040	170.666013	48.937869
1270.315274	179.652294	48.942874
1266.587316	164.432047	48.947879
1262.867563	171.118223	48.952884
1259.289906	173.824854	48.957889
1255.848108	169.189206	48.962893
1252.349192	172.128397	48.967898
1248.650557	163.526967	48.972903
1245.296378	162.349640	48.977908
1241.787963	161.957520	48.982913
1238.378858	163.122862	48.987917
1234.967359	162.779960	48.992922
1231.531068	161.132288	48.997927
1227.921489	164.607797	49.002932
1224.750585	162.535115	49.007937
1221.088494	163.104616	49.012941
1217.329762	161.286032	49.017946
1213.792074	160.109811	49.022951
1210.186498	172.066582	49.027956
1206.639272	163.499379	49.032961
1203.383564	169.747112	49.037965
1199.672099	172.376120	49.042970
1196.381002	150.173491	49.047975
1192.743889	165.045511	49.052980
1189.505692	166.875127	49.057985
1186.106067	157.433953	49.062989
1182.300287	165.716405	49.067994
1178.762880	166.209309	49.072999
1175.160204	171.697758	49.078004
1171.964820	150.425355	49.083009
1168.764863	155.566746	49.088013
1165.020014	162.381413	49.093018
1161.329902	153.979500	49.098023
1157.598597	166.099601	49.103028
1154.274714	159.502807	49.108033
1150.627060	159.127111	49.113037
1147.016287	166.072570	49.118042
1144.077763	157.916550	49.123047
1140.560337	162.109997	49.128052
1137.002853	151.947008	49.133057
1133.233278	154.104203	49.138061
1129.138322	157.123004	49.143066
1125.940672	154.696175	49.148071
1122.690112	165.180635	49.153076
1119.330075	145.957993	49.158081
1116.216375	154.259106	49.163085
1112.581656	165.229827	49.168090
1109.126897	152.080467	49.173095
1105.389829	156.801099	49.178100
1101.732674	143.210434	49.183105
1098.081671	155.406479	49.188109
1094.409884	151.986050	49.193114
1091.354721	154.466511	49.198119
1087.619641	159.470951	49.203124
1084.525350	165.987555	49.208129
1080.678938	157.540069	49.213133
1076.895363	157.210726	49.218138
1074.094438	151.858111	49.223143
1070.086353	157.220270	49.228148
1066.690218	147.384765	49.233153
1063.464137	160.214285	49.238157
1059.886439	164.590565	49.243162
1056.672589	151.754159	49.248167
1052.576192	155.031620	49.253172
1049.248912	159.442032	49.258177
1045.963367	149.125291	49.263181
1041.837225	152.567885	49.268186
1038.927979	165.728187	49.273191
1035.030296	157.002108	49.278196
1031.781440	145.294200	49.283201
1028.159055	158.112208	49.288205
1024.481802	159.205808	49.293210
1021.216516	152.178949	49.298215
1017.463689	154.938591	49.303220
1014.006637	155.702638	49.308225
1010.761521	152.016672	49.313229
1007.188942	154.986589	49.318234
1004.211303	159.258594	49.323239
1000.399815	157.370414	49.328244
996.505758	144.512678	49.333249
993.020418	143.168013	49.338253
989.377290	161.352362	49.343258
986.366915	149.109262	49.348263
982.856752	155.207306	49.353268
979.302556	155.771847	49.358273
975.732399	141.558993	49.363277
972.234149	149.941209	49.368282
968.718115	158.122250	49.373287
964.981502	149.892304	49.378292
961.067472	148.138085	49.383297
957.944699	152.585998	49.388301
954.862510	143.696527	49.393306
951.479651	142.566705	49.398311
947.972359	156.209636	49.403316
944.303887	146.432985	49.408321
940.694127	157.686245	49.413325
936.684990	161.638571	49.418330
933.560518	144.797575	49.423335
930.043707	142.214690	49.428340
926.342605	140.165970	49.433345
922.811595	142.196477	49.438349
919.206105	149.651898	49.443354
916.389264	143.332504	49.448359
912.831262	145.254216	49.453364
909.393175	143.514276	49.458369
905.763326	142.325421	49.463373
902.031252	155.909395	49.468378
899.074408	141.471610	49.473383
895.008440	146.495263	49.478388
891.412739	140.055680	49.483393
887.989657	136.460927	49.488397
884.386334	138.653645	49.493402
881.416891	135.878396	49.498407
877.258883	150.326584	49.503412
873.707608	138.426812	49.508417
870.834841	133.421293	49.513421
867.236879	142.642996	49.518426
863.809156	134.256164	49.523431
859.893451	145.336515	49.528436
856.458539	151.753769	49.533441
853.027988	135.758931	49.538445
849.232342	142.350192	49.543450
846.416626	134.089316	49.548455
842.685955	143.827206	49.553460
839.174519	141.060874	49.558465
835.255749	146.205769	49.563469
831.672167	145.178410	49.568474
828.444975	133.937050	49.573479
824.867443	136.642688	49.578484
821.628552	141.389419	49.583489
818.224413	135.238286	49.588493
814.700554	142.716479	49.593498
810.928959	143.670686	49.598503
807.579086	157.774145	49.603508
803.913443	135.602301	49.608513
800.362484	143.452663	49.613517
796.781310	152.782123	49.618522
793.725288	148.181098	49.623527
790.111663	136.291876	49.628532
786.580348	155.113977	49.633537
783.192148	138.206932	49.638541
779.517785	141.261249	49.643546
775.860615	139.420429	49.648551
772.075018	150.965806	49.653556
768.848872	134.979102	49.658561
765.455931	135.732194	49.663565
761.811974	148.681227	49.668570
758.971673	145.746690	49.673575
755.226774	148.206631	49.678580
751.035044	150.320588	49.683585
747.822477	147.425828	49.688589
744.352811	153.283284	49.693594
741.116632	134.163789	49.698599
737.442838	137.526428	49.703604
734.190030	138.978448	49.708609
730.441377	143.109447	49.713613
727.038387	130.025305	49.718618
723.441751	141.679286	49.723623
719.524360	152.325904	49.728628
716.259519	144.256068	49.733633
713.151482	134.055049	49.738637
709.755387	135.916583	49.743642
705.866928	138.026751	49.748647
702.393460	148.331128	49.753652
698.575209	140.149866	49.758657
695.298310	142.753239	49.763661
691.597864	144.929343	49.768666
688.539457	129.379167	49.773671
684.940209	137.514675	49.778676
681.511302	136.949406	49.783681
678.309856	137.431085	49.788685
674.214982	139.551783	49.793690
671.228098	137.758861	49.798695
667.289924	135.755759	49.803700
663.802765	138.106984	49.808705
660.072583	138.837297	49.813709
656.488367	143.217903	49.818714
653.555773	144.363731	49.823719
649.932827	136.050606	49.828724
646.210060	138.511093	49.833729
643.317624	138.289942	49.838733
639.416727	140.454095	49.843738
635.525342	130.745943	49.848743
632.293039	140.100424	49.853748
629.152364	137.001873	49.858753
625.759654	141.817995	49.863757
621.724865	142.052682	49.868762
618.448040	148.167501	49.873767
614.681812	143.042118	49.878772
610.978245	141.777603	49.883777
607.787503	139.227268	49.888781
604.123113	149.259068	49.893786
600.860437	138.927086	49.898791
597.480409	145.253801	49.903796
593.864817	149.540771	49.908801
590.511634	136.895590	49.913805
586.404596	141.628458	49.918810
583.201474	136.699543	49.923815
579.917580	140.500315	49.928820
576.562755	128.664982	49.933825
572.748775	136.625676	49.938829
568.921617	130.510130	49.943834
566.210670	124.967300	49.948839
562.150101	141.163677	49.953844
558.900023	137.317276	49.958849
555.179061	130.517884	49.963853
551.669060	142.958605	49.968858
548.375263	130.745030	49.973863
544.878752	128.887279	49.978868
541.170335	134.008436	49.983873
537.625577	130.090363	49.988877
533.577557	140.308972	49.993882
531.135370	133.340302	49.998887
527.343633	126.262477	50.003892
523.889187	125.778560	50.008897
520.470394	128.791290	50.013901
516.334700	138.547984	50.018906
513.402053	134.199804	50.023911
509.882967	136.181296	50.028916
506.101607	144.389983	50.033921
502.941258	135.418874	50.038925
498.993501	127.551951	50.043930
495.731661	133.050810	50.048935
492.117708	139.012713	50.053940
488.396385	129.956404	50.058945
485.144143	135.163638	50.063949
481.561057	142.149318	50.068954
478.070857	134.847094	50.073959
475.041908	129.410206	50.078964
471.269539	129.952751	50.083969
468.088343	128.681055	50.088973
464.231427	131.546382	50.093978
461.041171	126.882963	50.098983
456.967243	131.760882	50.103988
453.170477	122.254373	50.108993
450.461370	123.391193	50.113997
446.833038	129.483445	50.119002
443.427091	118.050875	50.124007
439.599943	133.387343	50.129012
435.805765	139.290157	50.134017
432.293464	127.120152	50.139021
428.711469	127.050494	50.144026
425.830114	122.561987	50.149031
422.729238	129.718912	50.154036
419.067139	130.152114	50.159041
415.167239	126.231417	50.164045
411.293604	123.035343	50.169050
407.947725	127.427309	50.174055
404.392666	129.937271	50.179060
400.894982	127.677185	50.184065
397.597168	127.334286	50.189069
394.036155	133.899740	50.194074
390.828973	123.348892	50.199079
387.112699	134.778012	50.204084
383.480717	129.979445	50.209089
380.066114	128.747537	50.214093
376.547103	138.555345	50.219098
373.272978	124.494094	50.224103
369.795203	130.836462	50.229108
366.201673	131.137317	50.234113
362.641372	124.463736	50.239117
358.861141	134.697779	50.244122
355.396268	131.223090	50.249127
351.925775	140.053418	50.254132
348.438400	130.992491	50.259137
345.006873	127.775707	50.264141
341.362535	140.155046	50.269146
338.184336	127.705075	50.274151
334.588119	133.873864	50.279156
330.873806	135.668787	50.284161
327.264318	124.210524	50.289165
323.949321	129.285640	50.294170
320.706489	134.999069	50.299175
317.016233	120.179389	50.304180
313.337417	135.397785	50.309185
310.212009	128.636305	50.314189
306.561057	130.045493	50.319194
303.217826	130.771666	50.324199
299.497056	133.763562	50.329204
296.124568	135.621305	50.334209
292.750067	137.747130	50.339213
288.800109	138.400115	50.344218
285.873608	140.992062	50.349223
282.009677	135.334516	50.354228
278.292232	134.302354	50.359233
274.643042	131.183723	50.364237
271.312374	135.270373	50.369242
268.026840	139.447039	50.374247
264.545084	124.606560	50.379252
260.847743	139.802392	50.384257
257.471441	126.808470	50.389261
253.876488	135.852962	50.394266
250.543020	131.661603	50.399271
247.167969	126.046335	50.404276
243.237396	134.298545	50.409281
240.060247	125.248391	50.414285
236.271081	128.108769	50.419290
233.019458	125.145958	50.424295
229.497063	125.887663	50.429300
225.804408	119.112325	50.434305
222.571656	124.838631	50.439309
218.847839	131.245597	50.444314
215.416424	128.411154	50.449319
211.561605	124.954512	50.454324
208.591855	130.073168	50.459329
205.355182	122.860935	50.464333
201.563499	129.735596	50.469338
198.221865	131.291735	50.474343
194.538595	135.966553	50.479348
190.725283	128.755287	50.484353
187.272889	124.946467	50.489357
183.529377	132.582485	50.494362
180.286263	124.002896	50.499367
177.276840	122.030442	50.504372
173.553643	130.266871	50.509377
170.159930	137.617801	50.514381
166.065422	137.821106	50.519386
162.673381	126.699050	50.524391
159.155559	131.502916	50.529396
155.550598	135.459240	50.534401
152.314171	117.071942	50.539405
149.155106	125.423328	50.544410
145.931044	121.289327	50.549415
141.888567	118.103468	50.554420
138.066535	125.079757	50.559425
134.977377	126.154805	50.564429
131.148563	121.881600	50.569434
127.856731	125.422360	50.574439
124.589822	127.136664	50.579444
120.703926	122.024571	50.584449
117.507048	118.313661	50.589453
113.503575	137.523764	50.594458
110.153505	125.186492	50.599463
106.729806	127.558198	50.604468
103.439709	131.741021	50.609473
100.462089	129.063101	50.614477
96.078528	133.024795	50.619482
92.626701	125.491248	50.624487
89.368846	119.626056	50.629492
86.328993	126.352865	50.634497
82.505360	131.077275	50.639501
78.485863	137.093376	50.644506
75.029948	130.856335	50.649511
71.731700	124.961226	50.654516
68.313492	128.976213	50.659521
64.720420	121.658106	50.664525
61.131185	133.113143	50.669530
57.609646	122.398988	50.674535
54.411947	122.682553	50.679540
50.679361	132.558747	50.684545
47.545864	132.679484	50.689549
43.941316	136.537046	50.694554
40.333885	132.403510	50.699559
36.982505	127.109716	50.704564
32.970577	137.516080	50.709569
29.903826	125.429584	50.714573
26.160752	132.659253	50.719578
22.926340	129.979019	50.724583
19.542021	114.830211	50.729588
15.767094	122.857140	50.734593
12.308817	116.051104	50.739597
8.513569	127.448655	50.744602
5.040134	122.089027	50.749607
1.555414	114.908240	50.754612