Thu Jun 16 11:19:44 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
-0.272787	82.387848	0.000000
-0.131103	89.041143	0.005005
0.189788	95.652099	0.010010
0.188000	90.413290	0.015014
0.307278	89.126282	0.020019
-0.057171	84.174311	0.025024
-0.261375	65.060646	0.030029
-0.386653	70.417640	0.035034
-0.585139	47.277387	0.040038
-0.691399	26.857885	0.045043
-1.496259	34.478608	0.050048
-1.730350	7.091740	0.055053
-1.880609	10.808586	0.060058
-1.935546	6.639113	0.065062
-2.422526	-10.746476	0.070067
-3.119197	5.156548	0.075072
-2.825509	-11.457049	0.080077
-3.409522	-24.752404	0.085082
-3.077088	-17.414851	0.090086
-3.960014	-20.996246	0.095091
-4.825196	-38.505758	0.100096
-4.851274	-32.041632	0.105101
-5.030921	-19.284689	0.110106
-5.229577	-20.894326	0.115110
-4.921819	-28.614964	0.120115
-5.186942	-21.767820	0.125120
-5.358668	-28.046820	0.130125
-6.072452	-44.392672	0.135130
-6.210041	-24.372742	0.140134
-6.511596	-30.109990	0.145139
-7.267013	-33.889733	0.150144
-7.552935	-27.178650	0.155149
-7.657119	-34.268294	0.160154
-8.112949	-33.436285	0.165158
-8.128687	-39.920409	0.170163
-8.391954	-27.242882	0.175168
-8.235851	-33.174932	0.180173
-8.588022	-18.970945	0.185178
-8.192915	-35.304428	0.190182
-8.205535	-38.837466	0.195187
-9.365124	-21.761046	0.200192
-9.676127	-36.995647	0.205197
-9.764643	-27.056406	0.210202
-10.288862	-18.998489	0.215206
-10.705069	-34.064668	0.220211
-11.123752	-22.356271	0.225216
-10.875727	-24.799551	0.230221
-11.145130	-25.362525	0.235226
-11.493128	-26.585917	0.240230
-11.388295	-32.058749	0.245235
-11.850883	-34.559900	0.250240
-11.761377	-33.117377	0.255245
-12.500450	-32.208372	0.260250
-12.840188	-35.229996	0.265254
-12.697869	-35.630359	0.270259
-13.438155	-34.316083	0.275264
-13.587427	-41.670456	0.280269
-13.406819	-32.460247	0.285274
-13.653628	-29.199905	0.290278
-14.171975	-35.937378	0.295283
-14.525222	-21.844300	0.300288
-14.612686	-27.563753	0.305293
-14.708433	-27.766929	0.310298
-14.724063	-19.704668	0.315302
-15.396715	-24.931619	0.320307
-16.007496	-24.139113	0.325312
-15.814762	-27.070664	0.330317
-16.098404	-28.588319	0.335322
-16.289355	-27.623789	0.340326
-16.297527	-36.937057	0.345331
-17.203148	-22.335097	0.350336
-17.472596	-32.245941	0.355341
-17.592682	-30.899990	0.360346
-18.098388	-29.113358	0.365350
-17.795381	-31.589203	0.370355
-17.742536	-24.641794	0.375360
-17.732756	-20.229755	0.380365
-18.710036	-30.689633	0.385370
-19.016713	-31.189326	0.390374
-18.986138	-32.705339	0.395379
-19.441888	-26.031992	0.400384
-19.501036	-24.292422	0.405389
-20.108637	-20.942759	0.410394
-20.625038	-19.888240	0.415398
-20.835992	-19.941858	0.420403
-21.195526	-22.839659	0.425408
-21.226879	-32.199213	0.430413
-21.179763	-22.008819	0.435418
-21.263391	-27.299469	0.440422
-21.016765	-36.759022	0.445427
-21.497832	-23.371501	0.450432
-21.810646	-31.510668	0.455437
-22.408537	-34.228988	0.460442
-22.885920	-16.825705	0.465446
-22.650917	-24.343526	0.470451
-23.024860	-22.349497	0.475456
-23.224516	-35.999777	0.480461
-23.898600	-31.971248	0.485466
-24.383064	-36.124675	0.490470
-24.069776	-39.167500	0.495475
-24.109653	-31.773362	0.500480
-24.286313	-35.823066	0.505485
-25.097491	-28.691043	0.510490
-25.613983	-32.909222	0.515494
-25.350311	-32.397072	0.520499
-25.859684	-25.020246	0.525504
-25.851080	-28.737822	0.530509
-25.956695	-27.247959	0.535514
-26.211040	-31.245168	0.540518
-26.656568	-37.154937	0.545523
-27.345424	-23.511010	0.550528
-27.488078	-28.884638	0.555533
-27.494160	-29.853283	0.560538
-27.662582	-25.598251	0.565542
-27.573044	-25.655458	0.570547
-27.833200	-25.320736	0.575552
-28.593686	-27.190208	0.580557
-28.948868	-23.548615	0.585562
-29.430357	-25.153339	0.590566
-29.214555	-22.775935	0.595571
-29.398292	-20.251114	0.600576
-29.260998	-24.888491	0.605581
-29.471020	-24.418810	0.610586
-30.441229	-30.462856	0.615590
-30.611334	-36.761257	0.620595
-30.999213	-16.502258	0.625600
-30.621200	-24.913931	0.630605
-30.615746	-33.769826	0.635610
-31.760834	-23.247946	0.640614
-31.701017	-35.184291	0.645619
-31.939165	-28.862399	0.650624
-32.368845	-35.101822	0.655629
-32.231239	-29.984233	0.660634
-32.558317	-27.031345	0.665638
-32.650774	-24.371066	0.670643
-33.375704	-33.403499	0.675648
-33.757687	-28.143217	0.680653
-33.907772	-27.044366	0.685658
-34.067815	-25.884086	0.690662
-33.791535	-39.378714	0.695667
-33.986267	-23.063334	0.700672
-34.675163	-27.538622	0.705677
-35.302455	-31.678015	0.710682
-35.514546	-28.701907	0.715686
-35.794385	-28.257979	0.720691
-35.914914	-30.697569	0.725696
-35.914441	-32.005776	0.730701
-35.744923	-17.060306	0.735706
-36.231456	-27.298713	0.740710
-36.825537	-40.826486	0.745715
-37.168401	-25.450174	0.750720
-36.998776	-24.734449	0.755725
-37.159175	-25.268280	0.760730
-37.438947	-27.159581	0.765734
-37.757465	-24.374634	0.770739
-38.565811	-27.828851	0.775744
-38.912313	-23.560075	0.780749
-38.534127	-27.466681	0.785754
-38.808855	-28.366168	0.790758
-38.672517	-35.402429	0.795763
-39.221440	-19.512209	0.800768
-39.857037	-29.903160	0.805773
-39.789787	-19.857070	0.810778
-40.105694	-24.857175	0.815782
-40.040283	-33.763721	0.820787
-41.486127	-28.766828	0.825792
-41.471159	-22.946092	0.830797
-41.192864	-32.478951	0.835802
-41.660931	-31.030407	0.840806
-41.768500	-25.605935	0.845811
-42.035753	-23.437459	0.850816
-41.857231	-20.544352	0.855821
-41.576884	-23.915479	0.860826
-42.451342	-31.071876	0.865830
-43.014146	-37.289297	0.870835
-43.422278	-14.114020	0.875840
-43.583279	-20.759217	0.880845
-43.424983	-29.421954	0.885850
-44.306384	-22.527027	0.890854
-44.693216	-26.826416	0.895859
-45.164480	-19.241315	0.900864
-44.929196	-31.067065	0.905869
-44.754621	-26.993218	0.910874
-45.260470	-22.631911	0.915878
-45.134936	-36.322611	0.920883
-45.220099	-16.251953	0.925888
-45.724436	-23.129067	0.930893
-45.970423	-30.794296	0.935898
-46.847203	-25.127674	0.940902
-46.861524	-33.430505	0.945907
-46.656521	-23.356377	0.950912
-47.206529	-17.611263	0.955917
-47.842915	-21.645962	0.960922
-48.284679	-19.745099	0.965926
-47.955127	-27.995159	0.970931
-48.406946	-30.678030	0.975936
-48.348663	-26.551324	0.980941
-48.534410	-26.703025	0.985946
-48.668600	-28.249619	0.990950
-48.729579	-32.672211	0.995955
-49.885955	-25.960519	1.000960
-49.734816	-32.099807	1.005965
-49.838058	-24.592694	1.010970
-50.106045	-29.604070	1.015974
-50.119981	-41.368500	1.020979
-50.788736	-29.907047	1.025984
-51.266990	-30.245991	1.030989
-51.211537	-36.539443	1.035994
-51.641316	-28.807995	1.040998
-51.161797	-35.087675	1.046003
-52.073889	-24.466383	1.051008
-53.048585	-27.349725	1.056013
-52.961396	-26.105704	1.061018
-52.660007	-34.853251	1.066022
-53.013673	-29.917088	1.071027
-53.167371	-27.153658	1.076032
-53.169742	-25.432252	1.081037
-53.147535	-34.417978	1.086042
-54.214996	-23.005954	1.091046
-54.439493	-34.762917	1.096051
-54.770604	-29.790922	1.101056
-54.999002	-29.561777	1.106061
-54.554681	-38.786254	1.111066
-54.917514	-28.264715	1.116070
-55.001498	-27.554826	1.121075
-55.942353	-22.870458	1.126080
-56.386891	-26.323928	1.131085
-56.237631	-31.222244	1.136090
-56.238523	-30.781796	1.141094
-56.245012	-26.657211	1.146099
-57.210050	-25.917042	1.151104
-57.868045	-25.602990	1.156109
-57.700496	-25.289823	1.161114
-57.977143	-24.832807	1.166118
-58.203504	-22.887632	1.171123
-58.306932	-25.641201	1.176128
-58.258458	-26.795550	1.181133
-58.204747	-39.723132	1.186138
-59.071199	-26.592942	1.191142
-59.182553	-33.957429	1.196147
-59.410170	-28.510159	1.201152
-59.964811	-30.707040	1.206157
-59.727664	-35.155914	1.211162
-60.586877	-33.622305	1.216166
-60.955149	-43.289606	1.221171
-61.368863	-28.216490	1.226176
-60.775347	-35.607593	1.231181
-60.945223	-29.418623	1.236186
-61.435782	-29.290976	1.241190
-61.456878	-37.875325	1.246195
-61.604011	-28.106148	1.251200
-62.450957	-38.750819	1.256205
-62.572062	-27.502596	1.261210
-63.300913	-22.086433	1.266214
-63.101665	-39.443520	1.271219
-62.993853	-36.849487	1.276224
-63.109350	-25.786080	1.281229
-63.794578	-43.629552	1.286234
-64.865610	-31.501808	1.291238
-64.611316	-28.060876	1.296243
-64.760769	-25.959617	1.301248
-64.861483	-38.572722	1.306253
-64.758962	-46.182975	1.311258
-65.077094	-32.077858	1.316262
-64.699503	-35.809157	1.321267
-65.566982	-30.983214	1.326272
-66.072967	-29.197520	1.331277
-66.094886	-28.541789	1.336282
-66.411937	-30.454846	1.341286
-66.265512	-24.678923	1.346291
-67.319573	-25.773982	1.351296
-67.420870	-32.067081	1.356301
-67.454467	-30.339923	1.361306
-67.935859	-20.419313	1.366310
-68.021457	-25.244682	1.371315
-68.264086	-24.203639	1.376320
-68.920804	-22.882253	1.381325
-69.002048	-25.035632	1.386330
-69.518578	-16.207715	1.391334
-69.420132	-21.803696	1.396339
-69.492051	-24.660237	1.401344
-69.920925	-22.705270	1.406349
-69.429893	-19.337201	1.411354
-69.654676	-25.834231	1.416358
-70.506816	-28.229267	1.421363
-71.132223	-24.792804	1.426368
-71.471111	-32.599633	1.431373
-71.354346	-25.679959	1.436378
-71.630753	-24.912817	1.441382
-71.430376	-34.725104	1.446387
-71.603794	-32.423565	1.451392
-72.564630	-27.369891	1.456397
-72.437226	-35.292354	1.461402
-72.975327	-19.335460	1.466406
-72.910744	-41.389260	1.471411
-73.113649	-27.648469	1.476416
-73.554270	-19.708152	1.481421
-74.110492	-36.059019	1.486426
-74.798338	-28.772760	1.491430
-74.506281	-33.666262	1.496435
-74.703299	-26.926368	1.501440
-74.315548	-25.627349	1.506445
-74.073240	-38.566072	1.511450
-74.944547	-31.382577	1.516454
-75.735355	-36.530204	1.521459
-75.943357	-32.642429	1.526464
-75.752007	-32.939517	1.531469
-76.201430	-33.066385	1.536474
-76.787292	-31.023915	1.541478
-77.179676	-40.221390	1.546483
-77.218699	-27.392798	1.551488
-77.649260	-42.348951	1.556493
-77.528773	-35.961439	1.561498
-77.767405	-28.489568	1.566502
-77.944413	-30.648034	1.571507
-77.615165	-28.615727	1.576512
-78.622912	-27.543138	1.581517
-79.205540	-19.201708	1.586522
-79.364870	-19.375828	1.591526
-79.272706	-30.164952	1.596531
-79.610269	-21.735972	1.601536
-79.459090	-27.974315	1.606541
-79.394204	-40.261706	1.611546
-80.890869	-21.996944	1.616550
-80.840809	-37.390840	1.621555
-81.002223	-33.766376	1.626560
-81.053006	-24.852265	1.631565
-81.051556	-37.868381	1.636570
-81.181533	-27.221365	1.641574
-81.464179	-35.514178	1.646579
-82.390770	-33.362912	1.651584
-82.769343	-27.349090	1.656589
-82.641810	-41.550936	1.661594
-82.941179	-32.173116	1.666598
-82.678391	-25.023051	1.671603
-82.752308	-36.988783	1.676608
-83.933886	-35.208337	1.681613
-84.018707	-36.086822	1.686618
-84.203797	-22.791726	1.691622
-84.328084	-39.299209	1.696627
-84.403900	-29.210051	1.701632
-84.556092	-18.779059	1.706637
-85.456091	-26.848306	1.711642
-85.672238	-34.891763	1.716646
-85.668058	-31.588849	1.721651
-86.022740	-27.886075	1.726656
-86.108754	-35.263131	1.731661
-85.732264	-34.520827	1.736666
-86.100236	-34.331457	1.741670
-86.863757	-38.874703	1.746675
-87.396911	-32.261273	1.751680
-87.520137	-25.763338	1.756685
-87.397236	-27.838581	1.761690
-87.942931	-30.667034	1.766694
-87.803023	-34.220543	1.771699
-88.275468	-28.821304	1.776704
-89.000522	-37.939925	1.781709
-89.115689	-36.619844	1.786714
-89.439751	-21.771081	1.791718
-89.263784	-36.177650	1.796723
-89.822759	-31.977839	1.801728
-89.361833	-28.145864	1.806733
-89.671226	-33.924818	1.811738
-90.411216	-31.270777	1.816742
-90.716617	-39.578964	1.821747
-90.807693	-24.901792	1.826752
-91.168972	-33.237249	1.831757
-90.751005	-34.313366	1.836762
-91.812945	-28.992994	1.841766
-92.118153	-29.919995	1.846771
-92.362258	-25.950389	1.851776
-92.537678	-22.181448	1.856781
-92.051230	-31.782247	1.861786
-92.464803	-26.078329	1.866790
-92.760424	-32.580417	1.871795
-93.372079	-31.959318	1.876800
-93.663775	-31.621650	1.881805
-93.960704	-24.953637	1.886810
-93.814783	-28.357201	1.891814
-94.216569	-29.640755	1.896819
-94.862296	-27.242216	1.901824
-95.542599	-29.978180	1.906829
-95.534681	-27.547088	1.911834
-95.723313	-24.527898	1.916838
-95.409162	-38.343383	1.921843
-95.613751	-29.043773	1.926848
-95.457276	-27.668157	1.931853
-95.613602	-38.442152	1.936858
-96.344629	-31.431595	1.941862
-96.852248	-35.659615	1.946867
-97.513677	-34.383520	1.951872
-97.404857	-28.876727	1.956877
-97.305918	-40.038194	1.961882
-98.453001	-29.647982	1.966886
-98.726996	-32.469248	1.971891
-98.490769	-42.317444	1.976896
-98.539094	-30.728472	1.981901
-98.730842	-30.013993	1.986906
-99.100665	-31.131469	1.991910
-99.003900	-31.009533	1.996915
-99.445963	-25.364561	2.006912
-99.383762	-32.160961	2.016909
-99.114035	-28.921499	2.026906
-98.230599	-24.052603	2.036902
-97.962633	-30.622678	2.046899
-97.487518	-28.821655	2.056896
-96.538431	-30.611559	2.066893
-96.248950	-26.256784	2.076890
-96.103263	-26.107778	2.086886
-94.856223	-19.814912	2.096883
-94.833342	-24.313530	2.106880
-94.721099	-25.970314	2.116877
-93.553847	-29.650264	2.126874
-93.192365	-28.139788	2.136870
-92.967196	-22.974468	2.146867
-92.637253	-24.236603	2.156864
-91.852241	-26.030111	2.166861
-91.326420	-33.828794	2.176858
-90.492784	-28.004621	2.186854
-90.484299	-29.890267	2.196851
-89.871180	-36.672022	2.206848
-88.947830	-33.643809	2.216845
-88.863226	-28.617602	2.226842
-88.677245	-30.628054	2.236838
-87.796597	-30.093184	2.246835
-87.586072	-20.969130	2.256832
-86.345360	-26.114513	2.266829
-85.607999	-27.348264	2.276826
-85.639676	-27.265317	2.286822
-85.643963	-26.760170	2.296819
-85.248528	-28.025177	2.306816
-84.371330	-37.276103	2.316813
-83.554158	-33.016046	2.326810
-82.821317	-25.464403	2.336806
-82.842760	-21.687020	2.346803
-82.497261	-21.206096	2.356800
-81.989456	-21.827605	2.366797
-81.072208	-27.729618	2.376794
-80.994547	-30.420488	2.386790
-80.260459	-28.580276	2.396787
-79.681495	-25.319020	2.406784
-79.275023	-26.004139	2.416781
-78.574968	-32.433544	2.426778
-77.874117	-27.904449	2.436774
-77.658525	-32.199078	2.446771
-77.314907	-25.973576	2.456768
-77.129880	-28.760967	2.466765
-76.412913	-25.597244	2.476762
-75.636308	-30.540867	2.486758
-74.805572	-22.766206	2.496755
-74.997761	-20.152278	2.506752
-74.454196	-21.795495	2.516749
-73.256419	-26.710291	2.526746
-73.177908	-31.002911	2.536742
-73.190134	-29.030862	2.546739
-72.416060	-24.037255	2.556736
-71.795441	-26.882213	2.566733
-71.328017	-28.038507	2.576730
-70.492850	-25.665934	2.586726
-69.845786	-21.520593	2.596723
-69.755541	-25.987672	2.606720
-69.801335	-23.402038	2.616717
-68.489869	-20.017408	2.626714
-68.052202	-26.641756	2.636710
-67.913564	-29.538386	2.646707
-67.244361	-26.598061	2.656704
-67.016341	-23.779665	2.666701
-65.998334	-22.518892	2.676698
-65.423587	-24.636068	2.686694
-65.471358	-25.458837	2.696691
-64.990617	-19.242954	2.706688
-63.996539	-23.314884	2.716685
-63.667395	-22.001608	2.726682
-63.406690	-19.409927	2.736678
-62.260038	-21.958606	2.746675
-62.019875	-25.045966	2.756672
-61.939669	-18.776827	2.766669
-61.479015	-24.998252	2.776666
-60.439685	-23.029296	2.786662
-60.347522	-24.953962	2.796659
-59.881270	-17.566627	2.806656
-58.900115	-30.820784	2.816653
-58.667107	-30.100447	2.826650
-58.447993	-27.533948	2.836646
-57.452020	-31.539562	2.846643
-57.287593	-31.569282	2.856640
-56.859682	-30.410521	2.866637
-55.715544	-30.364687	2.876634
-55.199819	-30.702278	2.886630
-55.514028	-30.164630	2.896627
-55.159054	-31.154170	2.906624
-54.429136	-31.468385	2.916621
-53.583073	-29.474848	2.926618
-52.632733	-21.751458	2.936614
-52.708175	-23.063700	2.946611
-52.458064	-24.878844	2.956608
-52.055989	-27.766855	2.966605
-50.903647	-32.261142	2.976602
-50.753038	-29.427976	2.986598
-50.215588	-17.527519	2.996595
-49.181076	-22.719474	3.006592
-48.813078	-21.496926	3.016589
-48.777449	-27.856730	3.026586
-48.734746	-25.572231	3.036582
-47.704564	-24.988230	3.046579
-47.401372	-29.278273	3.056576
-46.386165	-28.080106	3.066573
-45.672291	-31.716830	3.076570
-45.746557	-29.373687	3.086566
-45.739112	-29.841628	3.096563
-44.550354	-23.507163	3.106560
-44.250968	-26.342791	3.116557
-43.518419	-33.775632	3.126554
-42.785649	-29.212640	3.136550
-42.590305	-28.371642	3.146547
-42.530544	-25.359883	3.156544
-41.893647	-25.815536	3.166541
-41.063468	-35.191450	3.176538
-41.000905	-30.183972	3.186534
-39.907383	-36.512253	3.196531
-39.674085	-28.670018	3.206528
-39.318741	-35.132194	3.216525
-38.403721	-28.350064	3.226522
-38.321334	-33.529919	3.236518
-37.819536	-32.852570	3.246515
-36.938109	-35.499555	3.256512
-36.600873	-32.283198	3.266509
-36.360750	-37.495836	3.276506
-35.336940	-31.626676	3.286502
-35.028599	-29.279099	3.296499
-34.929191	-26.156147	3.306496
-34.153545	-22.479966	3.316493
-33.492534	-25.331054	3.326490
-33.250269	-28.021569	3.336486
-32.742689	-27.438965	3.346483
-31.935449	-26.161185	3.356480
-31.613537	-32.522615	3.366477
-31.303990	-29.911841	3.376474
-30.205993	-30.922281	3.386470
-30.233642	-31.836931	3.396467
-30.043930	-31.881893	3.406464
-28.735681	-33.403096	3.416461
-28.457106	-28.194294	3.426458
-28.363853	-25.981910	3.436454
-27.761180	-29.564301	3.446451
-26.931945	-25.081502	3.456448
-26.830316	-31.238060	3.466445
-25.779162	-30.377778	3.476442
-25.379780	-32.931764	3.486438
-25.502856	-28.037231	3.496435
-24.745488	-26.373180	3.506432
-23.490803	-28.948595	3.516429
-23.263904	-26.263413	3.526426
-23.477592	-28.938881	3.536422
-22.946497	-31.607685	3.546419
-22.001578	-34.938886	3.556416
-21.790969	-31.097368	3.566413
-20.954134	-35.365657	3.576410
-20.105359	-26.664008	3.586406
-20.513682	-33.291777	3.596403
-20.019941	-30.252859	3.606400
-18.936547	-36.719286	3.616397
-18.615730	-35.461528	3.626394
-18.041822	-31.264977	3.636390
-17.125869	-35.006906	3.646387
-16.902217	-34.271044	3.656384
-17.055539	-36.221273	3.666381
-16.649058	-35.094627	3.676378
-15.664289	-35.203017	3.686374
-14.817671	-26.394526	3.696371
-14.209555	-27.426935	3.706368
-13.962340	-30.212700	3.716365
-13.802827	-29.136117	3.726362
-13.363308	-27.471446	3.736358
-12.636143	-24.305250	3.746355
-12.215479	-29.285221	3.756352
-11.130630	-28.436135	3.766349
-10.843337	-27.268060	3.776346
-10.572253	-28.432897	3.786342
-10.611123	-28.197876	3.796339
-9.610475	-26.059879	3.806336
-9.280887	-34.544112	3.816333
-7.969947	-32.537257	3.826330
-8.039453	-27.346693	3.836326
-7.666609	-28.208795	3.846323
-7.649251	-29.446484	3.856320
-6.561431	-24.731956	3.866317
-6.136565	-23.568933	3.876314
-5.103465	-20.614007	3.886310
-4.808258	-12.532029	3.896307
-4.549592	-12.956981	3.906304
-4.298401	-19.184638	3.916301
-4.072093	-9.001492	3.926298
-3.506144	0.125487	3.936294
-2.598412	19.203811	3.946291
-2.644548	20.839347	3.956288
-2.220017	36.612411	3.966285
-1.589701	51.799501	3.976282
-0.980738	66.204685	3.986278
-0.599806	94.093578	3.996275
-0.275319	115.775401	4.006272
0.000000	123.945332	4.011277
0.098361	148.113574	4.016282
0.297587	148.803502	4.021286
0.569124	176.151408	4.026291
0.657169	172.142942	4.031296
1.236663	174.811092	4.036301
0.781255	186.959994	4.041306
0.937686	174.787715	4.046310
1.016057	183.839247	4.051315
1.109587	188.787802	4.056320
1.459033	198.181173	4.061325
1.585776	195.176628	4.066330
1.089245	187.613853	4.071334
1.276462	185.234652	4.076339
0.774835	181.556159	4.081344
1.032853	189.737076	4.086349
1.380561	201.924536	4.091354
1.368422	198.939192	4.096358
1.356419	201.504530	4.101363
1.197716	197.068028	4.106368
1.538740	202.274018	4.111373
1.612398	203.917183	4.116378
1.574151	198.439600	4.121382
1.357616	211.757073	4.126387
1.351135	204.196472	4.131392
1.865517	200.797177	4.136397
1.592561	198.074935	4.141402
1.041140	195.813159	4.146406
1.292337	189.708349	4.151411
1.577544	195.707471	4.156416
1.909442	203.869971	4.161421
1.138659	198.536726	4.166426
1.357522	193.616969	4.171430
1.521531	202.259841	4.176435
1.478414	204.641002	4.181440
1.907520	200.941683	4.186445
1.382396	198.807265	4.191450
1.653999	199.996956	4.196454
1.555024	189.481749	4.201459
1.562395	199.945426	4.206464
1.614322	199.658551	4.211469
1.490652	188.666485	4.216474
1.695850	205.572468	4.221478
1.429903	200.862754	4.226483
1.090436	202.504244	4.231488
0.746136	203.955142	4.236493
1.011303	204.182930	4.241498
1.309751	202.429855	4.246502
1.716949	227.287983	4.251507
1.773849	233.695692	4.256512
1.945893	232.083270	4.261517
1.938496	236.144249	4.266522
1.886825	220.308148	4.271526
1.385082	218.400518	4.276531
1.666762	227.986138	4.281536
2.206891	227.627661	4.286541
1.849385	225.900508	4.291546
1.803024	210.653495	4.296550
1.672153	212.970236	4.301555
1.822575	223.973706	4.306560
1.706617	231.196061	4.311565
1.583777	237.973735	4.316570
1.886188	243.488202	4.321574
1.671689	242.528725	4.326579
1.704601	241.792955	4.331584
1.911944	243.456849	4.336589
1.736362	236.774089	4.341594
1.939351	234.802086	4.346598
2.016352	244.169970	4.351603
1.871511	236.957483	4.356608
2.058074	239.408031	4.361613
1.600013	244.701892	4.366618
1.901450	237.943360	4.371622
2.023426	244.239888	4.376627
2.056561	238.691598	4.381632
2.236003	235.942238	4.386637
1.859845	247.287472	4.391642
2.076380	247.655691	4.396646
2.105435	244.610258	4.401651
2.055078	250.126495	4.406656
2.358078	247.396275	4.411661
1.911474	252.118118	4.416666
1.943261	244.773641	4.421670
2.130396	243.800474	4.426675
2.145528	242.823471	4.431680
2.186680	253.106587	4.436685
1.722551	249.368016	4.441690
1.795463	244.786381	4.446694
1.961624	263.760076	4.451699
2.110655	270.315849	4.456704
2.176888	268.658362	4.461709
2.070076	281.049642	4.466714
2.202630	275.957368	4.471718
2.325960	278.923486	4.476723
2.402746	282.383370	4.481728
2.738440	273.445394	4.486733
2.640773	275.337077	4.491738
2.579268	276.319005	4.496742
2.278443	260.819409	4.501747
1.926936	260.076036	4.506752
2.377474	265.316928	4.511757
2.264375	273.801713	4.516762
2.687593	272.791603	4.521766
2.654811	275.342234	4.526771
2.372698	265.067079	4.531776
2.258544	261.241073	4.536781
2.268026	269.625590	4.541786
2.386066	278.209114	4.546790
2.553810	282.314364	4.551795
2.655520	279.827242	4.556800
2.778753	273.188413	4.561805
2.367984	268.860729	4.566810
2.621517	252.503870	4.571814
2.497514	247.452819	4.576819
2.076610	254.005299	4.581824
2.548953	262.822184	4.586829
2.418488	265.162740	4.591834
2.521846	281.123947	4.596838
2.654915	275.570375	4.601843
2.405082	266.750474	4.606848
2.767386	275.053800	4.611853
2.714112	280.831868	4.616858
2.496589	276.778768	4.621862
2.647025	287.281804	4.626867
2.571322	275.080030	4.631872
2.556656	263.133265	4.636877
2.225078	288.313355	4.641882
2.572924	275.672124	4.646886
2.484830	266.577377	4.651891
2.583520	276.181034	4.656896
2.555925	269.432763	4.661901
2.412947	277.142620	4.666906
2.592119	281.040384	4.671910
2.745253	281.380014	4.676915
2.533178	288.576844	4.681920
2.855746	292.492744	4.686925
2.606196	322.734554	4.691930
2.826836	308.090007	4.696934
2.919292	316.747333	4.701939
3.040104	311.378286	4.706944
2.941275	308.316189	4.711949
3.008547	318.995869	4.716954
2.788981	302.046973	4.721958
2.661355	291.453167	4.726963
2.664600	313.603513	4.731968
3.110540	306.946955	4.736973
2.813286	317.053704	4.741978
3.338995	314.565370	4.746982
3.085257	316.777336	4.751987
2.965070	306.102675	4.756992
3.139065	297.699778	4.761997
2.548288	294.623679	4.767002
2.806297	292.750900	4.772006
2.928675	312.190538	4.777011
2.981408	316.757766	4.782016
3.450290	312.755585	4.787021
2.582427	307.407267	4.792026
2.741593	304.843463	4.797030
2.955144	314.690980	4.802035
2.721761	313.561874	4.807040
3.075391	311.344275	4.812045
3.309375	324.769020	4.817050
3.154599	314.059423	4.822054
3.275845	317.948024	4.827059
3.115055	310.754515	4.832064
3.172772	306.491464	4.837069
2.878475	319.312622	4.842074
2.917768	315.784735	4.847078
3.011568	308.494203	4.852083
3.173468	308.344239	4.857088
3.524018	308.556636	4.862093
3.196148	321.080964	4.867098
3.045237	306.274563	4.872102
3.034385	316.848470	4.877107
3.016826	325.912683	4.882112
3.371241	333.698812	4.887117
3.294547	344.424597	4.892122
3.521090	339.384152	4.897126
3.204557	333.931397	4.902131
3.154905	340.297861	4.907136
3.442240	342.758409	4.912141
3.258961	347.734508	4.917146
3.581055	354.768610	4.922150
3.717447	345.300994	4.927155
3.501522	346.018792	4.932160
3.446307	331.075799	4.937165
3.422003	331.812639	4.942170
3.244172	321.978270	4.947174
3.257999	342.806111	4.952179
3.416991	344.982925	4.957184
3.636030	326.531015	4.962189
3.535878	348.974734	4.967194
3.714862	344.045538	4.972198
3.662462	335.708741	4.977203
3.517777	338.649412	4.982208
3.516416	327.327157	4.987213
3.471381	336.771794	4.992218
3.574858	342.959940	4.997222
3.435505	348.054270	5.002227
3.346692	346.122681	5.007232
3.458465	335.423873	5.012237
3.066286	351.852786	5.017242
3.543376	344.847052	5.022246
3.338138	345.201611	5.027251
3.490051	348.671884	5.032256
3.746569	343.943859	5.037261
3.293964	342.083142	5.042266
3.717021	349.794895	5.047270
3.767203	353.751384	5.052275
3.600482	346.750822	5.057280
3.807193	344.738432	5.062285
3.459537	356.702143	5.067290
3.375524	351.656387	5.072294
3.538337	367.230106	5.077299
3.720981	381.857414	5.082304
3.646452	376.671470	5.087309
3.585045	375.106590	5.092314
3.899851	375.755823	5.097318
3.869641	369.933036	5.102323
3.973845	382.214054	5.107328
3.962419	377.188554	5.112333
3.726124	377.912483	5.117338
3.544637	378.253744	5.122342
3.375296	382.257173	5.127347
3.732403	374.296239	5.132352
3.915012	384.179596	5.137357
3.623448	384.223152	5.142362
3.952343	372.160631	5.147366
3.632700	377.334782	5.152371
3.855753	394.849886	5.157376
3.963315	389.732404	5.162381
4.273339	401.146277	5.167386
4.298472	392.213284	5.172390
3.898451	379.270548	5.177395
3.812330	389.728099	5.182400
4.245450	376.119283	5.187405
3.822790	390.442535	5.192410
4.422412	391.249412	5.197414
3.971951	378.784120	5.202419
3.774834	390.975046	5.207424
4.096027	400.815091	5.212429
4.128304	407.919112	5.217434
4.496282	394.039481	5.222438
4.245036	393.911028	5.227443
3.806886	381.818985	5.232448
4.140739	394.221590	5.237453
3.935710	407.049772	5.242458
4.388477	405.562603	5.247462
4.370771	397.742423	5.252467
4.186009	402.885808	5.257472
4.569743	389.757112	5.262477
3.997940	401.254262	5.267482
4.382041	399.560806	5.272486
4.449737	404.482919	5.277491
4.190735	395.800011	5.282496
4.205754	389.399610	5.287501
4.165391	405.515218	5.292506
4.317109	405.284558	5.297510
4.417189	400.310571	5.302515
4.509930	419.408862	5.307520
4.529639	412.777807	5.312525
4.503864	398.955448	5.317530
4.608934	384.663681	5.322534
4.599922	377.900058	5.327539
4.317980	375.513317	5.332544
4.479549	373.308310	5.337549
4.325205	379.211046	5.342554
4.612022	383.897558	5.347558
4.263317	374.584080	5.352563
4.212188	381.109937	5.357568
4.566770	365.943115	5.362573
4.456594	383.109969	5.367578
4.391764	387.049464	5.372582
4.457179	395.587588	5.377587
4.520742	404.372663	5.382592
4.800502	406.481582	5.387597
4.425913	405.368109	5.392602
4.293218	395.897081	5.397606
4.399782	398.208156	5.402611
4.302194	414.848411	5.407616
4.624596	401.272768	5.412621
4.468726	406.129027	5.417626
4.489817	410.355525	5.422630
4.595082	399.445342	5.427635
4.638589	406.960677	5.432640
4.744687	409.977615	5.437645
4.329941	419.183387	5.442650
4.424514	400.171860	5.447654
4.416733	405.132689	5.452659
4.391652	422.396315	5.457664
4.554285	419.378002	5.462669
5.060670	437.382824	5.467674
4.555536	432.766333	5.472678
4.673476	436.228034	5.477683
4.481024	444.388919	5.482688
4.837363	444.148615	5.487693
4.816263	446.425447	5.492698
5.032783	439.787507	5.497702
5.041157	446.972349	5.502707
4.610957	453.530099	5.507712
4.929604	444.845626	5.512717
4.712374	442.423221	5.517722
4.567521	447.695087	5.522726
4.894165	439.205029	5.527731
4.846470	440.526824	5.532736
5.077691	437.195483	5.537741
4.835192	442.999455	5.542746
5.026152	443.748674	5.547750
5.093258	447.487024	5.552755
4.888931	456.691490	5.557760
5.047423	439.163107	5.562765
5.139195	451.254645	5.567770
5.143072	443.509504	5.572774
5.000406	446.106439	5.577779
5.017809	454.961028	5.582784
5.341613	449.816078	5.587789
5.197980	437.889602	5.592794
5.221171	447.247364	5.597798
5.140183	441.453066	5.602803
5.126906	437.793550	5.607808
4.999664	437.167404	5.612813
4.943981	445.796502	5.617818
5.123772	445.082819	5.622822
5.167529	445.184318	5.627827
4.818093	445.450733	5.632832
5.302191	438.387664	5.637837
5.099745	455.453629	5.642842
5.419379	441.916686	5.647846
5.307615	438.784977	5.652851
5.133908	458.674472	5.657856
5.564836	446.631631	5.662861
5.446926	445.296381	5.667866
5.277491	441.605153	5.672870
5.128306	437.611059	5.677875
5.110012	448.747443	5.682880
5.213119	444.944976	5.687885
5.059669	455.089218	5.692890
5.127464	450.906544	5.697894
5.418392	441.371896	5.702899
5.316971	447.670896	5.707904
5.633296	438.669038	5.712909
5.368643	447.978671	5.717914
5.230798	447.428663	5.722918
5.598077	446.284834	5.727923
5.606798	452.623940	5.732928
5.156417	451.225244	5.737933
5.396775	451.956928	5.742938
5.065715	449.163739	5.747942
5.117060	448.481344	5.752947
5.073807	453.305492	5.757952
5.238341	449.647172	5.762957
5.327729	446.964649	5.767962
5.063260	444.644858	5.772966
5.233498	469.437074	5.777971
5.242636	478.662314	5.782976
5.565211	468.665738	5.787981
5.170613	478.039384	5.792986
5.350881	475.323784	5.797990
5.374965	465.901586	5.802995
5.353731	479.734361	5.808000
5.462000	476.584830	5.813005
5.167412	484.724632	5.818010
5.438974	498.296137	5.823014
5.823094	495.939202	5.828019
5.761565	499.034864	5.833024
5.702847	496.592668	5.838029
5.612668	493.531768	5.843034
5.598661	505.207431	5.848038
5.839598	503.146252	5.853043
5.426880	490.888222	5.858048
5.798749	494.461877	5.863053
5.668480	510.412898	5.868058
5.823130	505.102516	5.873062
5.953673	500.661733	5.878067
5.726196	502.889708	5.883072
6.034036	503.068421	5.888077
6.012849	508.355289	5.893082
5.581672	492.087551	5.898086
5.815996	506.280143	5.903091
5.642888	499.040436	5.908096
5.813897	501.081212	5.913101
5.730802	502.955519	5.918106
5.974771	504.614178	5.923110
6.001991	500.194119	5.928115
5.479242	512.987386	5.933120
6.176148	502.308872	5.938125
6.242892	504.357408	5.943130
6.025748	514.111767	5.948134
5.921032	504.296473	5.953139
5.922959	506.699933	5.958144
6.212622	502.761851	5.963149
5.877037	507.940851	5.968154
5.734895	505.106073	5.973158
5.968121	498.578703	5.978163
5.872008	497.793605	5.983168
6.178474	498.295744	5.988173
6.419135	502.249010	5.993178
5.851149	503.638342	5.998182
6.455946	498.213125	6.003187
6.179419	503.128521	6.008192
6.024824	505.090609	6.013197
6.095099	506.425570	6.018202
6.100999	501.370431	6.023206
6.319035	494.835905	6.028211
6.231670	508.935747	6.033216
6.242432	499.392607	6.038221
6.043001	500.057865	6.043226
5.962412	487.263212	6.048230
6.324071	495.754804	6.053235
6.206923	497.101993	6.058240
5.677352	481.218317	6.063245
5.902469	491.294795	6.068250
6.172547	509.834995	6.073254
6.296306	507.200254	6.078259
5.964590	499.640769	6.083264
6.201725	510.056920	6.088269
5.972031	512.765227	6.093274
6.375539	509.013436	6.098278
6.270864	505.212440	6.103283
5.964985	514.467857	6.108288
6.260666	511.004697	6.113293
6.179766	511.312469	6.118298
6.074817	503.927817	6.123302
5.965747	489.838562	6.128307
5.976977	494.455518	6.133312
6.051272	503.129564	6.138317
6.331001	512.963511	6.143322
5.980262	500.171266	6.148326
6.408655	504.124684	6.153331
5.914039	511.544904	6.158336
6.301043	503.381255	6.163341
6.377028	502.459491	6.168346
5.876988	487.080195	6.173350
6.048257	469.380667	6.178355
5.771185	492.070382	6.183360
5.924922	501.734636	6.188365
5.874949	502.989333	6.193370
6.067313	502.893033	6.198374
6.004540	505.636008	6.203379
6.157046	506.451371	6.208384
6.527253	501.673729	6.213389
6.074353	503.767196	6.218394
6.057837	507.892202	6.223398
6.201928	503.391268	6.228403
6.334328	509.089902	6.233408
6.034773	503.007417	6.238413
6.147766	519.882516	6.243418
5.986090	514.827046	6.248422
5.835961	511.942878	6.253427
6.134843	511.783791	6.258432
6.412411	505.864610	6.263437
6.103738	505.282748	6.268442
5.838645	515.258525	6.273446
6.576449	506.570652	6.278451
6.008342	502.706345	6.283456
6.072876	501.227781	6.288461
6.368456	503.354126	6.293466
6.150393	496.913469	6.298470
6.359582	484.756200	6.303475
5.814552	489.736088	6.308480
5.927299	482.360261	6.313485
6.451326	493.628935	6.318490
5.905930	503.639976	6.323494
6.030433	487.246871	6.328499
5.998776	503.760604	6.333504
6.017410	504.193597	6.338509
6.220013	498.657559	6.343514
6.060054	504.591361	6.348518
6.112581	508.354036	6.353523
5.924262	509.291132	6.358528
6.092319	512.446723	6.363533
6.191620	516.970306	6.368538
6.015655	505.424015	6.373542
6.446407	508.520903	6.378547
6.170979	517.047545	6.383552
6.234798	519.370536	6.388557
6.366455	508.606267	6.393562
5.956000	487.001538	6.398566
6.037581	477.281755	6.403571
5.592670	483.581989	6.408576
5.964901	497.799730	6.413581
5.959570	508.962429	6.418586
5.594074	510.535541	6.423590
5.992605	505.371417	6.428595
5.988457	516.819733	6.433600
6.233139	510.682527	6.438605
6.153588	504.948445	6.443610
6.127794	514.659147	6.448614
6.288454	503.439524	6.453619
6.087527	513.727007	6.458624
6.268628	510.229113	6.463629
6.378342	510.968281	6.468634
6.385723	513.102002	6.473638
6.205949	511.643782	6.478643
5.940543	512.659815	6.483648
6.036265	501.821380	6.488653
5.951583	517.451739	6.493658
6.169453	513.726777	6.498662
6.227814	503.374282	6.503667
6.041693	513.291527	6.508672
6.511919	506.305600	6.513677
6.451519	500.334637	6.518682
5.949403	502.810638	6.523686
6.120162	503.312315	6.528691
6.169963	508.326900	6.533696
6.116846	497.716691	6.538701
5.882455	500.027496	6.543706
5.876832	503.477568	6.548710
6.379574	496.150347	6.553715
6.093548	514.818462	6.558720
6.583993	512.852886	6.563725
6.121251	486.528186	6.568730
5.769539	488.802144	6.573734
6.178529	500.728140	6.578739
6.021122	509.511020	6.583744
6.093879	503.087514	6.588749
6.014099	519.605171	6.593754
5.936821	508.189864	6.598758
6.288310	504.111436	6.603763
5.733065	518.334284	6.608768
6.042707	500.752439	6.613773
6.104392	512.703775	6.618778
5.784883	520.546121	6.623782
5.874811	501.697921	6.628787
5.774769	518.056832	6.633792
5.976400	518.470043	6.638797
5.871760	517.173930	6.643802
5.777645	517.677943	6.648806
5.834780	509.342485	6.653811
5.525938	519.091382	6.658816
6.133041	534.634766	6.663821
6.415901	539.563985	6.668826
6.220108	532.478463	6.673830
6.389960	529.876944	6.678835
6.135998	523.467367	6.683840
6.050187	510.429876	6.688845
5.866481	525.642320	6.693850
6.049633	527.192644	6.698854
6.237602	530.718167	6.703859
5.949222	546.877573	6.708864
6.295360	531.559263	6.713869
6.541650	533.219416	6.718874
6.087961	530.273137	6.723878
6.131596	512.173191	6.728883
6.064942	513.760750	6.733888
6.228561	513.088508	6.738893
6.039703	515.001209	6.743898
6.169939	514.544425	6.748902
6.079637	505.913489	6.753907
6.006278	516.540581	6.758912
6.038571	527.776198	6.763917
6.241383	512.489879	6.768922
5.677837	518.184940	6.773926
6.117858	512.832724	6.778931
6.197510	523.463935	6.783936
6.360777	528.920897	6.788941
6.271200	515.355619	6.793946
6.242609	514.752729	6.798950
6.050908	508.181529	6.803955
5.833958	513.327016	6.808960
5.892305	505.393089	6.813965
5.928196	509.419363	6.818970
5.895925	530.540094	6.823974
6.401109	531.664378	6.828979
6.275279	540.409894	6.833984
6.136422	529.559791	6.838989
6.186086	519.592892	6.843994
5.721195	521.949487	6.848998
6.387961	526.559147	6.854003
6.187085	518.381059	6.859008
6.104778	510.747797	6.864013
6.267540	512.172642	6.869018
6.024011	511.221103	6.874022
6.572003	507.282850	6.879027
5.605163	509.096909	6.884032
5.993117	517.558912	6.889037
6.203403	513.652886	6.894042
6.131264	519.872097	6.899046
5.905746	510.977300	6.904051
5.855122	517.856520	6.909056
6.157419	528.351791	6.914061
6.305421	535.832261	6.919066
6.172184	530.857425	6.924070
6.247763	520.798438	6.929075
5.872541	516.641996	6.934080
6.139278	516.581254	6.939085
6.497908	512.714841	6.944090
6.035582	512.621465	6.949094
6.296728	508.241376	6.954099
6.170839	517.395525	6.959104
6.099585	511.082731	6.964109
6.090139	510.891330	6.969114
6.025874	521.171428	6.974118
6.426372	504.232309	6.979123
6.460558	512.441904	6.984128
6.257466	517.214547	6.989133
6.012484	494.159439	6.994138
6.142119	507.244056	6.999142
5.872577	508.612680	7.004147
6.140812	504.043283	7.009152
6.448000	510.805951	7.014157
6.599798	512.535781	7.019162
6.092723	507.174829	7.024166
6.245556	509.414443	7.029171
6.099811	524.189583	7.034176
5.992704	516.879175	7.039181
6.026987	515.186788	7.044186
5.810909	524.287279	7.049190
6.017786	516.591228	7.054195
6.070277	515.931727	7.059200
6.367263	507.293122	7.064205
6.191906	518.808998	7.069210
5.983981	515.874199	7.074214
6.288402	509.562463	7.079219
5.987826	516.538926	7.084224
6.138702	511.191282	7.089229
6.313488	518.540643	7.094234
6.026284	519.167822	7.099238
6.130846	511.722498	7.104243
5.974562	518.164273	7.109248
5.958608	513.763381	7.114253
6.025880	510.374963	7.119258
6.070485	514.309527	7.124262
6.408401	517.843713	7.129267
5.982958	518.949037	7.134272
6.145653	515.200242	7.139277
6.196569	514.048013	7.144282
5.849264	522.116043	7.149286
6.102068	520.141099	7.154291
5.649289	517.576967	7.159296
6.174850	516.924726	7.164301
6.125037	518.097906	7.169306
6.016168	521.610426	7.174310
6.311484	506.708386	7.179315
5.994826	521.583392	7.184320
5.953892	523.374571	7.189325
5.850516	515.685396	7.194330
5.952142	523.082464	7.199334
6.225766	517.702497	7.204339
5.903146	515.869310	7.209344
6.204384	521.732823	7.214349
6.524643	511.090105	7.219354
5.912521	519.872958	7.224358
6.234424	526.405206	7.229363
5.925636	513.366380	7.234368
6.341265	512.035395	7.239373
6.022495	510.124818	7.244378
5.938827	515.107398	7.249382
6.218826	516.056978	7.254387
6.082018	517.291890	7.259392
6.165962	504.312676	7.264397
6.023427	513.424685	7.269402
5.826907	520.711888	7.274406
6.390388	508.495361	7.279411
6.372765	516.696551	7.284416
6.390245	513.282522	7.289421
6.490170	502.950487	7.294426
5.951194	510.910388	7.299430
6.131176	511.825984	7.304435
6.125109	514.829513	7.309440
6.185023	513.156667	7.314445
6.690310	513.326627	7.319450
6.555712	514.249418	7.324454
6.265443	515.843051	7.329459
6.224686	519.443563	7.334464
6.194827	503.334135	7.339469
6.365796	485.449164	7.344474
5.795113	494.123637	7.349478
5.963315	494.021859	7.354483
6.189374	501.711194	7.359488
6.073561	498.957108	7.364493
6.259280	501.093715	7.369498
5.832262	490.037022	7.374502
5.990518	496.690222	7.379507
6.219131	511.862435	7.384512
6.354010	506.609285	7.389517
6.021713	504.726989	7.394522
6.122737	503.762414	7.399526
6.251888	494.715982	7.404531
6.042497	496.881774	7.409536
6.169693	480.404669	7.414541
5.874199	487.835973	7.419546
5.946760	506.812908	7.424550
6.443602	504.586513	7.429555
6.045936	507.094977	7.434560
6.251336	499.239454	7.439565
6.116895	482.498170	7.444570
5.820753	481.638790	7.449574
6.013505	490.228338	7.454579
5.877266	504.351445	7.459584
6.008892	505.944713	7.464589
6.381808	519.925289	7.469594
5.880284	517.668142	7.474598
6.396212	514.185061	7.479603
6.307989	515.355414	7.484608
6.217049	510.088673	7.489613
5.951975	496.371872	7.494618
5.958376	496.634337	7.499622
6.304184	501.322384	7.504627
6.220974	508.487662	7.509632
5.661510	492.649463	7.514637
5.802777	504.097910	7.519642
5.929947	514.361462	7.524646
5.961875	510.162698	7.529651
5.874669	513.949552	7.534656
5.935455	514.631496	7.539661
6.166928	513.638456	7.544666
5.741969	508.574899	7.549670
5.891790	502.906700	7.554675
5.748466	511.296869	7.559680
5.685145	510.072854	7.564685
6.210508	518.035046	7.569690
5.973314	531.946867	7.574694
6.734808	519.022895	7.579699
6.437685	519.008275	7.584704
6.094350	523.617832	7.589709
6.371598	506.991990	7.594714
5.994292	515.587557	7.599718
6.148975	518.380035	7.604723
6.057663	518.475639	7.609728
5.835362	513.181081	7.614733
6.119551	514.177027	7.619738
6.056879	513.728346	7.624742
6.165709	504.133777	7.629747
6.150423	515.989806	7.634752
5.931227	518.301063	7.639757
5.989645	511.698592	7.644762
5.849808	512.727910	7.649766
6.281728	511.335237	7.654771
6.344877	508.277704	7.659776
6.430164	514.048746	7.664781
6.424974	508.208749	7.669786
6.390101	520.002017	7.674790
6.589610	504.924615	7.679795
6.205626	505.728794	7.684800
6.462929	523.159460	7.689805
6.624275	505.785322	7.694810
6.237140	491.538389	7.699814
6.091437	484.026210	7.704819
5.846668	487.350845	7.709824
6.092875	482.740698	7.714829
6.114155	483.002677	7.719834
5.895920	483.058977	7.724838
6.015143	492.253208	7.729843
6.083938	508.941443	7.734848
6.056032	501.065675	7.739853
6.380478	507.260780	7.744858
6.018357	511.555566	7.749862
5.999387	513.642833	7.754867
6.217272	514.050990	7.759872
6.339449	507.098211	7.764877
6.285229	498.479272	7.769882
5.759980	489.639938	7.774886
6.085558	489.162318	7.779891
6.175188	498.425964	7.784896
6.206830	507.290858	7.789901
6.099349	485.356471	7.794906
5.824451	492.441247	7.799910
6.308378	506.105622	7.804915
6.270235	508.942788	7.809920
5.978414	483.628308	7.814925
6.091022	497.568418	7.819930
5.886594	510.281850	7.824934
6.371638	507.864531	7.829939
6.025332	511.700220	7.834944
6.005239	509.733872	7.839949
6.007207	510.316520	7.844954
6.259036	513.816392	7.849958
6.108318	520.938669	7.854963
6.165216	517.278290	7.859968
5.847304	511.350963	7.864973
6.308065	515.985587	7.869978
6.123194	519.052505	7.874982
6.347707	500.305387	7.879987
5.866070	498.134734	7.884992
5.782371	507.001720	7.889997
6.223574	514.728217	7.895002
6.026512	512.123603	7.900006
6.204566	503.488869	7.905011
6.233917	512.787445	7.910016
5.971859	513.528955	7.915021
6.265665	520.260395	7.920026
6.064555	523.149455	7.925030
6.398014	520.006604	7.930035
6.413707	492.279648	7.935040
6.273706	496.433444	7.940045
6.412101	484.733407	7.945050
5.797765	487.119033	7.950054
5.825237	483.275486	7.955059
5.860700	485.872391	7.960064
6.184755	496.657647	7.965069
6.232763	483.443075	7.970074
5.898068	492.390501	7.975078
6.272977	497.914587	7.980083
6.249206	481.694271	7.985088
6.058521	478.061991	7.990093
6.125318	474.753768	7.995098
6.188680	486.881797	8.000102
6.106630	479.498897	8.005107
6.042297	485.244832	8.010112
6.255714	488.338751	8.015130
6.235249	479.209297	8.020147
5.933356	485.982703	8.025165
5.952159	482.263941	8.030182
6.287144	478.722903	8.035200
6.067923	477.612923	8.040218
6.017955	482.244936	8.045235
5.708525	489.594567	8.050253
6.266056	508.170929	8.055270
6.214796	512.369395	8.060288
6.151768	511.432576	8.065306
6.418708	514.345052	8.070323
6.206880	520.692256	8.075341
6.106461	497.145705	8.080358
5.963259	502.220995	8.085376
6.224317	507.505802	8.090394
6.359234	512.058068	8.095411
6.187454	517.851128	8.100429
6.694067	505.451943	8.105446
6.304250	494.732381	8.110464
5.864654	488.467178	8.115482
6.346698	479.002766	8.120499
5.802329	491.780064	8.125517
5.923715	494.826507	8.130534
5.951884	499.244276	8.135552
5.911575	519.383809	8.140570
6.320331	504.381453	8.145587
6.170359	523.382561	8.150605
6.210729	508.676364	8.155622
6.317704	517.608627	8.160640
6.087421	514.280556	8.165658
6.424077	510.280765	8.170675
6.104038	521.105072	8.175693
6.322982	519.228925	8.180710
6.363896	514.225368	8.185728
6.389091	512.943133	8.190746
6.329339	520.917130	8.195763
6.671852	521.440342	8.200781
6.428742	522.237657	8.205798
6.342900	514.880042	8.210816
6.338772	517.678881	8.215834
5.966263	508.007415	8.220851
5.824353	518.938574	8.225869
6.165917	513.722572	8.230886
6.378874	522.832560	8.235904
6.204042	533.728136	8.240922
6.617049	512.604864	8.245939
6.406934	511.731124	8.250957
6.309960	519.645832	8.255974
6.276812	520.323821	8.260992
6.128157	513.407798	8.266010
6.419118	522.186162	8.271027
6.541526	510.765237	8.276045
6.296063	508.109419	8.281062
6.035458	522.337277	8.286080
6.280136	518.789995	8.291098
6.637489	507.832014	8.296115
6.447095	515.992918	8.301133
6.612280	516.467695	8.306150
6.432236	506.394815	8.311168
6.318179	522.491274	8.316186
6.487404	524.181176	8.321203
6.328558	515.481867	8.326221
6.230359	507.071790	8.331238
6.324442	518.632416	8.336256
5.884762	528.442459	8.341274
6.583496	540.083261	8.346291
6.332248	554.326331	8.351309
6.349163	552.193370	8.356326
6.878211	541.525037	8.361344
6.595552	544.511908	8.366362
6.645889	530.174243	8.371379
6.373292	522.063199	8.376397
6.261119	526.692515	8.381414
6.658930	514.718502	8.386432
6.147100	537.678920	8.391450
6.213157	542.583352	8.396467
6.643468	546.913521	8.401485
6.670880	548.333812	8.406502
6.780839	547.003321	8.411520
6.470587	540.126290	8.416538
6.633390	532.569341	8.421555
6.507797	528.984645	8.426573
6.555110	527.203579	8.431590
6.936755	519.947804	8.436608
6.267083	522.107864	8.441626
6.437268	515.966343	8.446643
6.312255	537.018727	8.451661
6.582564	546.947823	8.456678
7.097010	550.749235	8.461696
6.721952	533.774247	8.466714
6.619447	526.943682	8.471731
6.595235	527.956838	8.476749
6.537987	512.840872	8.481766
6.975971	504.269764	8.486784
6.222681	523.083230	8.491802
6.638663	517.226809	8.496819
6.357304	521.912620	8.501837
6.156124	529.192424	8.506854
6.376875	529.204272	8.511872
6.492440	546.650715	8.516890
6.398201	541.969324	8.521907
6.323574	546.806276	8.526925
6.554465	553.781961	8.531942
6.883301	556.369320	8.536960
6.653952	547.319315	8.541978
6.958074	546.206392	8.546995
7.025758	564.911990	8.552013
6.546816	556.701491	8.557030
6.921105	542.729486	8.562048
6.619663	561.575689	8.567066
6.986319	552.951296	8.572083
6.823171	543.271287	8.577101
6.628703	550.427182	8.582119
6.668052	546.997864	8.587136
6.673372	549.354883	8.592154
6.784040	549.344085	8.597171
6.856400	549.641918	8.602189
6.771124	551.633868	8.607207
6.830781	541.355442	8.612224
6.638458	553.077081	8.617242
6.765310	548.957750	8.622259
6.752923	555.656972	8.627277
6.812058	557.811536	8.632295
7.012288	545.219397	8.637312
6.912075	553.258058	8.642330
6.812078	543.105601	8.647347
6.900878	544.809485	8.652365
6.769272	531.995873	8.657383
6.667205	524.502085	8.662400
6.433865	538.724173	8.667418
6.820033	537.055283	8.672435
6.777033	545.643230	8.677453
6.201284	553.813516	8.682471
6.857756	544.007015	8.687488
6.618127	552.288257	8.692506
6.767938	551.019276	8.697523
6.939331	552.455529	8.702541
6.471730	561.350709	8.707559
6.718823	546.648397	8.712576
6.614051	546.124593	8.717594
6.260520	543.422467	8.722611
6.898732	559.527594	8.727629
7.005316	580.854696	8.732647
6.841354	564.275411	8.737664
6.852754	554.711206	8.742682
6.933840	572.090064	8.747699
7.127721	566.406619	8.752717
6.897187	559.789776	8.757735
7.026757	543.098929	8.762752
6.778953	553.558933	8.767770
6.442644	549.161489	8.772787
6.885127	569.658519	8.777805
6.833974	579.275872	8.782823
7.059669	568.289517	8.787840
7.204057	578.747411	8.792858
7.087787	576.188022	8.797875
7.217492	577.155278	8.802893
6.996571	563.149950	8.807911
6.980483	553.607115	8.812928
6.632063	562.297993	8.817946
7.131399	568.579751	8.822963
6.928313	577.150576	8.827981
6.812454	586.885593	8.832999
6.968524	569.595281	8.838016
6.990062	575.290288	8.843034
7.222018	575.550037	8.848051
7.414380	573.923995	8.853069
7.025909	552.550517	8.858087
6.815722	553.221748	8.863104
7.249801	564.284087	8.868122
6.983311	566.055248	8.873139
6.934345	557.367968	8.878157
7.102288	571.846443	8.883175
6.928206	569.645063	8.888192
6.758486	586.031636	8.893210
7.152661	585.787902	8.898227
7.172371	575.592615	8.903245
7.161394	579.039317	8.908263
7.236944	581.521715	8.913280
7.260032	577.691025	8.918298
7.124418	565.366334	8.923315
7.106540	562.524404	8.928333
6.671695	571.227207	8.933351
7.190030	579.661595	8.938368
7.259842	580.950399	8.943386
6.854459	579.779560	8.948403
7.094021	577.765676	8.953421
6.955243	577.252608	8.958439
7.256567	582.293728	8.963456
7.451740	584.062404	8.968474
7.128932	571.487696	8.973491
7.289453	583.497435	8.978509
7.192362	589.514746	8.983527
7.405403	577.129674	8.988544
7.587743	586.382626	8.993562
7.286730	567.098484	8.998579
6.880567	550.841761	9.003597
7.153240	567.396889	9.008615
7.486974	566.551949	9.013632
7.264644	552.767094	9.018650
6.982127	553.144730	9.023667
7.362472	560.778456	9.028685
7.075296	568.534502	9.033703
7.418723	566.878872	9.038720
7.180368	573.068309	9.043738
7.432779	571.681507	9.048755
7.309828	554.364107	9.053773
7.010550	558.608394	9.058791
7.546333	551.134160	9.063808
7.347186	555.969157	9.068826
7.322752	558.593640	9.073843
7.206992	541.863923	9.078861
7.005739	555.312869	9.083879
7.335981	575.387009	9.088896
7.397548	574.495134	9.093914
7.324821	586.020791	9.098931
7.562211	579.803879	9.103949
7.325519	561.942388	9.108967
7.310118	548.967560	9.113984
7.279871	550.512709	9.119002
6.832581	554.785883	9.124019
7.315103	563.898288	9.129037
7.040481	576.236277	9.134055
7.170635	580.989409	9.139072
7.148659	583.239942	9.144090
7.071323	579.580343	9.149107
7.306578	590.790791	9.154125
7.145323	579.518738	9.159143
7.210697	577.006876	9.164160
7.158495	574.976457	9.169178
7.128302	584.573128	9.174195
7.411424	594.865812	9.179213
7.604781	604.967571	9.184231
7.305303	585.431825	9.189248
7.474816	592.588700	9.194266
7.500376	605.905247	9.199283
7.686849	586.567484	9.204301
7.349755	588.780544	9.209319
7.149074	590.995171	9.214336
7.858248	592.407210	9.219354
7.461374	587.431495	9.224371
7.717525	584.206943	9.229389
7.355465	590.275913	9.234407
7.248612	579.668259	9.239424
7.438359	590.456097	9.244442
7.433870	618.519648	9.249459
7.781764	615.039720	9.254477
7.584140	601.140033	9.259495
7.560035	594.654580	9.264512
7.660720	587.919616	9.269530
7.369576	588.769646	9.274547
7.047591	587.068889	9.279565
7.580287	605.643962	9.284583
7.418877	612.148980	9.289600
7.902374	605.433408	9.294618
7.636404	618.057640	9.299635
7.908331	613.735614	9.304653
7.685658	598.715784	9.309671
7.486485	596.731004	9.314688
7.942851	591.252942	9.319706
7.346345	585.894160	9.324723
7.601576	580.554536	9.329741
7.541702	603.065636	9.334759
7.697438	586.601671	9.339776
7.832671	592.272090	9.344794
7.726104	597.974596	9.349811
7.656015	587.960839	9.354829
7.458594	585.714799	9.359847
7.462837	588.427738	9.364864
7.629370	586.704113	9.369882
7.682947	607.646980	9.374899
8.099484	612.597924	9.379917
7.740918	608.587923	9.384935
7.694803	586.969276	9.389952
7.768150	575.406441	9.394970
7.357240	590.900092	9.399987
7.407330	579.489394	9.405005
7.799662	598.467401	9.410023
7.799057	608.526427	9.415040
8.193501	605.964608	9.420058
7.808428	590.923109	9.425075
8.267157	587.925853	9.430093
7.876606	587.085173	9.435111
7.734526	580.410307	9.440128
7.919831	575.601624	9.445146
7.885009	589.820376	9.450163
7.624422	588.706695	9.455181
7.625182	589.999235	9.460199
7.622168	586.006453	9.465216
7.635843	588.303152	9.470234
7.658910	594.552920	9.475251
7.735791	582.260016	9.480269
7.837422	585.894466	9.485287
7.724837	583.968986	9.490304
8.088664	577.401523	9.495322
7.684927	589.203786	9.500339
7.813700	572.126798	9.505357
7.732563	580.286213	9.510375
7.945367	584.846984	9.515392
8.010210	573.409841	9.520410
7.613988	583.077333	9.525427
7.601827	581.299988	9.530445
7.939320	591.186717	9.535463
8.101045	602.968661	9.540480
8.306534	589.108548	9.545498
7.857891	587.932557	9.550515
7.721060	577.291283	9.555533
7.568798	589.554054	9.560551
7.905154	598.292092	9.565568
8.163134	600.430728	9.570586
8.009508	619.064620	9.575603
8.287658	587.132914	9.580621
8.014654	587.130708	9.585639
7.779533	577.413959	9.590656
8.153547	575.027337	9.595674
7.642085	577.489343	9.600691
7.907410	582.372862	9.605709
7.937612	595.034827	9.610727
8.077862	592.784156	9.615744
8.299563	591.839740	9.620762
7.622162	599.004908	9.625779
8.097121	596.454681	9.630797
8.174970	597.049580	9.635815
7.942968	602.542745	9.640832
8.082939	602.788962	9.645850
8.128422	594.530550	9.650867
7.791092	595.982877	9.655885
7.680819	593.904288	9.660903
7.845858	605.128711	9.665920
8.005632	602.163832	9.670938
7.701941	612.454309	9.675955
8.118820	602.532573	9.680973
8.309085	604.085078	9.685991
8.076115	611.204656	9.691008
8.274039	597.642085	9.696026
7.834392	609.150259	9.701043
7.904541	611.045877	9.706061
8.219806	607.564553	9.711079
7.896526	605.112582	9.716096
8.221696	605.602943	9.721114
7.984347	602.771294	9.726131
7.727215	610.456366	9.731149
8.053894	609.617313	9.736167
8.140212	604.396128	9.741184
8.473543	600.178009	9.746202
8.296357	613.202345	9.751219
8.088731	599.624425	9.756237
8.381870	604.149686	9.761255
8.140318	612.310534	9.766272
8.363751	599.492514	9.771290
8.407386	608.547381	9.776307
8.255394	611.466815	9.781325
8.366858	601.319524	9.786343
8.252631	608.740673	9.791360
8.319093	603.782756	9.796378
8.172403	605.527827	9.801395
8.158760	610.621793	9.806413
8.038361	609.531687	9.811431
7.715157	602.659032	9.816448
8.114899	605.306714	9.821466
8.059879	621.421664	9.826483
8.354382	622.126696	9.831501
8.488879	635.452230	9.836519
8.208861	628.851997	9.841536
8.435331	631.366637	9.846554
8.465017	637.474313	9.851571
8.758458	630.380179	9.856589
8.574837	603.713780	9.861607
8.453123	603.978739	9.866624
8.454215	600.462147	9.871642
8.112415	605.657182	9.876659
8.304560	595.428957	9.881677
8.324734	601.435554	9.886695
8.447031	608.366526	9.891712
8.577824	609.282237	9.896730
8.326734	600.794639	9.901747
8.162043	604.456573	9.906765
7.962613	600.149857	9.911783
8.044364	611.418456	9.916800
8.880062	624.473410	9.921818
8.930288	629.762201	9.926835
8.741072	616.835818	9.931853
8.679689	606.865680	9.936871
8.314734	608.547627	9.941888
8.479666	596.172753	9.946906
8.280275	605.363135	9.951923
8.403186	603.707138	9.956941
8.466325	596.766705	9.961959
8.316552	593.455325	9.966976
8.532774	593.316574	9.971994
8.483057	601.873681	9.977011
8.210081	597.361644	9.982029
8.453899	609.794363	9.987047
8.181027	637.341290	9.992064
8.605067	628.532504	9.997082
8.443241	628.013402	10.002099
8.658803	636.369633	10.007117
8.832562	631.991890	10.012135
8.786128	638.924288	10.017152
8.850034	621.890438	10.022170
8.995860	616.136782	10.027187
8.790603	611.249056	10.032205
8.729778	600.911186	10.037223
8.790930	613.886885	10.042240
8.629568	597.831735	10.047258
8.367920	613.953172	10.052275
8.544103	601.118357	10.057293
8.713021	605.031202	10.062311
8.550641	608.220703	10.067328
8.385655	601.005923	10.072346
8.676256	605.551875	10.077363
8.550229	616.815944	10.082381
8.931902	601.710903	10.087399
8.724348	621.514403	10.092416
8.522910	607.171728	10.097434
8.345140	599.550284	10.102451
8.260285	617.010344	10.107469
8.728910	626.611109	10.112487
8.842650	636.300441	10.117504
8.732780	639.670998	10.122522
8.934392	640.616928	10.127539
8.530195	636.527765	10.132557
8.844253	640.778668	10.137575
8.867462	651.597121	10.142592
9.225430	629.986721	10.147610
8.848315	614.844789	10.152627
8.476482	617.696932	10.157645
8.561393	615.885238	10.162663
8.773928	633.293909	10.167680
8.984131	629.517503	10.172698
9.127600	627.494498	10.177715
8.432282	612.521763	10.182733
8.607210	617.856071	10.187751
8.632914	643.870795	10.192768
9.006428	643.998907	10.197786
9.009596	632.712436	10.202803
8.799896	644.762050	10.207821
8.881844	634.362087	10.212839
8.929086	634.442857	10.217856
8.872572	634.799285	10.222874
9.009278	629.626741	10.227891
8.207091	630.810585	10.232909
8.754930	633.463222	10.237927
9.040051	634.510191	10.242944
8.814091	638.024611	10.247962
8.782607	637.457006	10.252979
8.550392	633.862351	10.257997
8.777676	632.433248	10.263015
8.957254	637.259611	10.268032
9.014319	634.897606	10.273050
8.985001	639.658708	10.278067
8.926103	634.537282	10.283085
9.027857	629.053943	10.288103
8.805652	635.969136	10.293120
9.025735	621.368834	10.298138
9.047593	628.971007	10.303155
8.573446	635.176507	10.308173
8.911377	637.544408	10.313191
9.144094	658.983129	10.318208
9.383906	651.333097	10.323226
9.011244	637.098496	10.328243
8.751764	647.063741	10.333261
9.097967	652.050135	10.338279
9.438061	651.940707	10.343296
9.083076	644.893497	10.348314
9.160619	643.400967	10.353331
8.646641	638.187847	10.358349
9.099595	640.275079	10.363367
9.096074	657.145874	10.368384
9.233926	666.345214	10.373402
9.192307	669.489285	10.378419
8.862348	669.818573	10.383437
9.097668	658.128142	10.388455
9.102648	655.100366	10.393472
9.242137	669.155373	10.398490
9.498136	655.159418	10.403507
9.123166	667.388005	10.408525
9.439090	649.675102	10.413543
9.252338	647.847877	10.418560
9.132483	639.074253	10.423578
9.180612	629.519282	10.428595
9.255765	635.794508	10.433613
9.528732	636.917585	10.438631
9.334935	629.814421	10.443648
9.349058	636.537440	10.448666
9.271444	633.137764	10.453683
9.020722	630.152938	10.458701
9.160655	617.539608	10.463719
9.291656	624.837875	10.468736
9.234780	628.773082	10.473754
9.342360	628.019831	10.478771
9.188104	623.205547	10.483789
9.478609	625.825526	10.488807
9.246706	627.019536	10.493824
8.952041	635.114484	10.498842
9.296016	636.299729	10.503859
9.103915	654.537838	10.508877
9.465413	658.359139	10.513895
9.415797	657.194352	10.518912
9.261863	653.646587	10.523930
9.455641	661.201866	10.528947
9.164847	663.589729	10.533965
9.402755	652.762681	10.538983
9.724962	657.586245	10.544000
9.498409	664.868239	10.549018
9.438475	650.151224	10.554035
9.378594	661.509787	10.559053
9.419107	659.825677	10.564071
9.462294	662.222214	10.569088
9.291401	666.827719	10.574106
9.661435	659.789602	10.579123
9.337136	660.153676	10.584141
9.443617	657.238235	10.589159
9.871512	650.089006	10.594176
9.863399	662.753127	10.599194
9.914584	645.377818	10.604211
9.094559	631.957064	10.609229
9.475912	635.519913	10.614247
9.161022	628.644691	10.619264
9.433703	643.916396	10.624282
9.686209	648.770369	10.629299
9.805039	654.735491	10.634317
9.750022	655.692637	10.639335
9.690335	634.859770	10.644352
9.422000	639.421048	10.649370
9.508006	626.860511	10.654387
9.403916	644.278613	10.659405
9.953543	649.810311	10.664423
9.585188	645.635907	10.669440
9.274105	642.880793	10.674458
9.522800	652.232345	10.679475
9.849823	656.616714	10.684493
9.861019	656.450833	10.689511
9.959862	653.467081	10.694528
9.758671	645.924568	10.699546
9.810972	628.133921	10.704563
9.138056	629.293057	10.709581
9.587555	632.949347	10.714599
9.952924	650.683696	10.719616
9.700735	660.922887	10.724634
9.880842	646.129995	10.729651
9.546988	631.944487	10.734669
9.720399	644.681724	10.739687
10.050452	636.343495	10.744704
9.572174	635.246890	10.749722
9.923672	633.489053	10.754739
9.394423	631.156532	10.759757
9.624410	639.030457	10.764775
10.016741	648.925776	10.769792
9.716399	652.860778	10.774810
9.979062	654.765622	10.779827
9.675555	658.870603	10.784845
9.529112	661.995290	10.789863
9.740797	660.279547	10.794880
9.295302	667.725651	10.799898
9.802613	651.249966	10.804915
9.449960	654.543937	10.809933
9.629003	663.690218	10.814951
10.053208	653.999477	10.819968
9.754764	661.279573	10.824986
9.850845	658.332884	10.830003
9.820299	656.183642	10.835021
9.749696	662.734884	10.840039
10.002032	665.613589	10.845056
9.748282	658.921716	10.850074
9.680363	654.229151	10.855091
9.698081	664.436141	10.860109
9.561102	673.634159	10.865127
10.156927	685.562695	10.870144
9.892149	688.082162	10.875162
10.143721	694.192457	10.880179
10.585603	689.776490	10.885197
10.472117	666.886730	10.890215
10.220285	660.796686	10.895232
9.940358	658.040061	10.900250
9.883344	645.917137	10.905267
9.948050	650.637020	10.910285
9.807947	653.882484	10.915303
9.839936	645.337945	10.920320
9.975951	667.049892	10.925338
9.829011	656.572505	10.930355
9.987224	652.943732	10.935373
10.352248	678.060480	10.940391
10.195868	668.648315	10.945408
9.993618	662.709789	10.950426
10.253885	665.693068	10.955443
9.898136	672.719108	10.960461
10.045510	679.613002	10.965479
10.527619	685.058941	10.970496
10.339784	677.852426	10.975514
10.157687	666.418136	10.980531
10.448344	648.874240	10.985549
10.107010	651.442467	10.990567
10.299092	653.911819	10.995584
10.269371	654.818730	11.000602
10.136867	648.304917	11.005619
10.126327	651.408422	11.010637
10.114191	651.348935	11.015655
10.167816	667.117206	11.020672
10.092095	657.499925	11.025690
10.017420	650.444474	11.030707
10.228858	677.812148	11.035725
10.338123	684.394884	11.040743
10.727350	676.190823	11.045760
10.364289	676.591611	11.050778
10.266940	660.191532	11.055795
10.008486	655.363360	11.060813
10.223890	669.863214	11.065831
10.599302	671.106936	11.070848
10.482735	671.065888	11.075866
10.391060	655.638701	11.080883
10.210856	652.659241	11.085901
10.126650	659.088148	11.090919
10.587665	666.192064	11.095936
10.195694	670.685118	11.100954
10.198617	667.106213	11.105971
10.474335	672.037739	11.110989
10.430279	684.615709	11.116007
10.641939	685.492082	11.121024
10.383865	686.147614	11.126042
10.037598	676.254719	11.131059
10.620472	690.742381	11.136077
10.385742	696.856874	11.141095
10.428742	687.735899	11.146112
10.329023	702.518227	11.151130
10.565103	689.519238	11.156147
10.559171	687.713592	11.161165
10.408325	690.650368	11.166183
10.682285	685.327589	11.171200
10.503722	694.693091	11.176218
10.449163	695.913399	11.181235
10.496458	685.868470	11.186253
10.570714	696.533172	11.191271
10.831111	693.738521	11.196288
10.538026	684.762341	11.201306
11.023516	691.148584	11.206323
10.633359	668.170514	11.211341
10.304042	670.712058	11.216359
10.561026	681.541890	11.221376
10.800245	684.041541	11.226394
10.243238	683.253653	11.231411
10.655973	679.779134	11.236429
10.621706	684.384504	11.241447
10.826728	689.417858	11.246464
10.777952	694.156311	11.251482
10.701931	689.618194	11.256499
10.729858	680.211483	11.261517
10.739774	691.235172	11.266535
10.799161	683.442040	11.271552
10.828961	674.066710	11.276570
10.885924	674.729815	11.281587
10.641071	662.051912	11.286605
10.656303	657.046057	11.291623
10.943959	648.994496	11.296640
10.378555	652.795383	11.301658
10.343790	678.249404	11.306675
10.940646	688.938053	11.311693
10.637210	699.472395	11.316711
11.169999	674.063596	11.321728
10.846092	690.894773	11.326746
11.266492	685.538348	11.331763
10.841467	665.311475	11.336781
10.348377	664.486850	11.341799
10.724942	671.320823	11.346816
10.712252	680.871560	11.351834
10.943655	679.266118	11.356851
11.313062	672.545261	11.361869
10.617206	682.297362	11.366887
10.977519	678.668644	11.371904
10.932031	680.499440	11.376922
10.955054	672.779829	11.381939
11.123956	676.402004	11.386957
10.684291	688.405813	11.391975
10.652532	678.685112	11.396992
10.612991	687.612952	11.402010
10.866558	682.568196	11.407027
10.759366	680.444311	11.412045
10.405790	693.107880	11.417063
10.647202	684.788799	11.422080
10.633158	678.050122	11.427098
10.793890	701.865398	11.432115
10.945110	693.842264	11.437133
10.862103	703.238625	11.442151
11.403419	703.506298	11.447168
11.282035	702.471159	11.452186
10.988659	700.154460	11.457203
11.200408	698.344725	11.462221
11.102630	703.647077	11.467239
10.805661	689.869512	11.472256
11.044747	707.562603	11.477274
11.075112	703.234023	11.482291
11.545135	708.814127	11.487309
10.881937	706.561888	11.492327
11.315649	713.888996	11.497344
11.183328	711.402795	11.502362
11.078996	707.337174	11.507379
11.505281	707.578984	11.512397
11.195996	695.714990	11.517415
11.032811	683.215957	11.522432
11.007541	694.442668	11.527450
11.249496	701.729033	11.532467
11.384784	716.729576	11.537485
10.983488	715.731639	11.542503
11.132356	705.052905	11.547520
11.462832	706.763317	11.552538
11.305166	717.159924	11.557555
11.314000	700.637747	11.562573
11.258183	709.505310	11.567591
10.941030	715.464369	11.572608
11.094858	701.894822	11.577626
10.941015	711.126058	11.582643
11.307175	702.945179	11.587661
11.161407	711.583758	11.592679
11.560685	702.028085	11.597696
11.504632	714.123314	11.602714
11.192716	714.219940	11.607731
11.621785	703.544598	11.612749
11.464337	703.882969	11.617767
11.171800	710.184053	11.622784
11.092705	705.677733	11.627802
11.176806	711.952987	11.632819
11.792929	710.359147	11.637837
11.450949	719.644308	11.642855
11.397421	714.836572	11.647872
11.428677	703.574831	11.652890
11.339839	714.947076	11.657907
11.426548	705.468738	11.662925
11.429042	706.048540	11.667943
11.589942	703.933193	11.672960
11.708195	705.511287	11.677978
11.675525	715.669857	11.682995
11.409097	705.377505	11.688013
11.129803	712.983334	11.693031
11.435428	711.676882	11.698048
11.098264	703.298806	11.703066
11.412700	718.147525	11.708083
12.012195	736.646181	11.713101
11.627447	720.940061	11.718119
11.238821	707.442438	11.723136
11.771508	722.381252	11.728154
11.504090	737.669384	11.733171
11.744242	733.494674	11.738189
11.769040	740.949398	11.743207
11.614012	729.168527	11.748224
12.025235	734.529661	11.753242
11.579973	728.854749	11.758259
11.431675	717.560969	11.763277
11.118359	721.055894	11.768295
11.512490	732.854443	11.773312
11.531567	743.554572	11.778330
11.625155	741.036741	11.783347
11.951818	723.327588	11.788365
11.930301	741.307930	11.793383
11.748759	737.642388	11.798400
12.084402	728.494579	11.803418
11.995400	734.533047	11.808435
12.287512	737.755617	11.813453
12.021295	728.097739	11.818471
11.533414	712.835951	11.823488
12.071835	717.972555	11.828506
12.067667	713.494295	11.833523
11.675435	707.373408	11.838541
11.749273	717.714733	11.843559
11.327399	715.519838	11.848576
11.653054	726.606904	11.853594
11.602010	741.001968	11.858611
11.976167	738.730040	11.863629
11.965472	738.877362	11.868647
12.028094	734.955863	11.873664
11.821326	740.962426	11.878682
11.923622	742.954401	11.883699
11.989198	742.051719	11.888717
12.279845	742.549069	11.893735
12.486682	732.236943	11.898752
12.124809	732.108012	11.903770
11.793917	745.963119	11.908787
12.111485	734.696553	11.913805
12.247997	738.593926	11.918823
12.055466	727.814142	11.923840
11.805421	732.408933	11.928858
12.037927	739.181522	11.933875
12.074074	736.776413	11.938893
12.481742	734.129333	11.943911
12.181182	735.518127	11.948928
11.918573	723.582532	11.953946
12.077510	726.037102	11.958963
12.359948	722.386211	11.963981
11.862593	731.206598	11.968999
11.893491	729.099249	11.974016
12.230880	729.587594	11.979034
12.118652	738.600691	11.984051
12.394805	728.364793	11.989069
12.124109	731.235079	11.994087
12.235409	740.318107	11.999104
12.463959	727.088780	12.004122
12.181008	730.984026	12.009139
12.085472	732.728136	12.014157
12.620085	725.135924	12.019175
12.283806	733.755023	12.024192
12.748500	732.422676	12.029210
12.042742	712.034102	12.034227
12.305727	699.741053	12.039245
12.281453	707.705053	12.044263
12.007727	709.901950	12.049280
12.213646	716.608760	12.054298
11.913801	717.552441	12.059315
12.075100	733.493501	12.064333
12.217750	726.176652	12.069351
12.376281	732.436072	12.074368
12.424910	726.430181	12.079386
12.189015	731.275045	12.084403
12.387467	729.679373	12.089421
12.491431	725.635712	12.094439
12.529731	737.193617	12.099456
12.273197	724.028316	12.104474
12.191216	734.101561	12.109491
12.277793	733.754258	12.114509
12.312294	726.985592	12.119527
12.191182	738.774625	12.124544
12.418590	729.508803	12.129562
12.304461	728.643494	12.134579
12.287290	746.738358	12.139597
12.590415	754.007553	12.144615
12.741590	755.624692	12.149632
12.572299	753.650895	12.154650
12.581321	777.990870	12.159667
12.811709	753.205526	12.164685
12.731103	740.143495	12.169703
12.645865	742.871248	12.174720
12.539851	724.765672	12.179738
12.546883	731.547867	12.184755
12.432115	739.944179	12.189773
12.908261	741.674806	12.194791
12.666041	737.919606	12.199808
13.078060	729.160379	12.204826
12.656825	734.443864	12.209843
12.581203	725.951310	12.214861
12.652865	730.979064	12.219879
12.627745	728.583096	12.224896
12.916286	727.487398	12.229914
12.629567	735.814898	12.234931
12.484599	726.970584	12.239949
12.834051	720.984262	12.244967
12.701082	742.126119	12.249984
12.736047	742.628032	12.255002
12.548903	750.320895	12.260019
12.511003	756.601273	12.265037
12.898405	742.396551	12.270055
12.287208	757.198901	12.275072
12.625935	762.358975	12.280090
12.572241	759.557861	12.285107
12.677782	755.198145	12.290125
12.699734	753.248344	12.295143
12.712577	759.359836	12.300160
13.018561	761.978659	12.305178
12.774689	755.304497	12.310195
12.800035	762.726962	12.315213
12.849014	760.177728	12.320231
12.920764	774.003618	12.325248
13.280911	770.953735	12.330266
13.178848	765.679782	12.335283
13.229201	759.295221	12.340301
13.289952	756.773367	12.345319
13.009278	753.227333	12.350336
13.280271	736.777225	12.355354
13.224550	750.920265	12.360371
13.368468	750.456026	12.365389
13.119952	741.885361	12.370407
13.062592	747.508447	12.375424
13.244985	744.249799	12.380442
13.253323	747.935329	12.385459
13.259150	737.085955	12.390477
13.237736	742.470860	12.395495
12.942014	744.342326	12.400512
13.132938	752.239690	12.405530
13.164108	748.762770	12.410547
13.246812	753.329346	12.415565
13.516927	747.617590	12.420583
13.187424	741.821594	12.425600
12.939486	745.614028	12.430618
13.156442	741.181978	12.435635
12.783556	744.340067	12.440653
12.947543	748.713912	12.445671
12.901444	753.700909	12.450688
13.261448	749.750437	12.455706
12.946180	746.309709	12.460723
12.956650	756.334626	12.465741
13.121391	743.777220	12.470759
13.449988	763.011487	12.475776
13.593244	758.606275	12.480794
13.608023	754.287242	12.485811
13.394214	755.490377	12.490829
13.336235	741.477836	12.495847
13.136021	756.850730	12.500864
13.107728	743.790679	12.505882
13.092513	758.442485	12.510899
13.495057	777.117902	12.515917
13.566862	783.685025	12.520935
13.568566	781.473557	12.525952
13.712481	774.633453	12.530970
13.603061	754.670685	12.535987
13.278935	753.645626	12.541005
13.498896	745.298468	12.546023
13.220311	748.796025	12.551040
13.214372	774.272503	12.556058
13.780713	774.593020	12.561075
13.605155	782.750925	12.566093
14.053804	786.754671	12.571111
13.366241	770.369544	12.576128
13.456111	756.741240	12.581146
13.471747	762.447624	12.586163
13.524355	780.556385	12.591181
13.428457	778.223376	12.596199
13.335905	782.623388	12.601216
13.955322	783.545452	12.606234
13.731183	781.898273	12.611251
13.452601	790.812143	12.616269
13.732531	788.093759	12.621287
13.652918	789.156336	12.626304
13.718564	781.768343	12.631322
13.447392	781.209836	12.636339
13.379888	791.835838	12.641357
13.637443	771.983041	12.646375
13.305452	788.136458	12.651392
13.320774	783.315355	12.656410
13.635613	776.347515	12.661427
13.654817	789.725103	12.666445
13.599952	785.188874	12.671463
14.010154	796.409728	12.676480
13.981646	796.593551	12.681498
14.046921	793.596524	12.686515
13.655136	786.472865	12.691533
13.981070	779.441687	12.696551
13.940107	788.290013	12.701568
13.681376	782.276931	12.706586
14.142245	783.077488	12.711603
14.093837	796.826030	12.716621
14.149628	778.215395	12.721639
14.150384	791.476076	12.726656
14.217060	788.269803	12.731674
13.708947	778.614374	12.736691
13.542307	786.018192	12.741709
13.785865	785.459746	12.746727
13.971862	779.771227	12.751744
13.755225	784.938947	12.756762
13.871218	794.409150	12.761779
13.880083	806.387248	12.766797
13.895805	806.861246	12.771815
14.210346	808.160601	12.776832
14.200369	819.820229	12.781850
14.436714	807.544387	12.786867
14.120296	809.511291	12.791885
14.253854	812.143954	12.796903
14.318207	828.088143	12.801920
13.896415	814.594037	12.806938
14.198501	806.376654	12.811955
13.769586	810.374372	12.816973
13.885652	809.845849	12.821991
14.005505	808.843069	12.827008
14.190053	819.066186	12.832026
14.122242	815.643594	12.837043
13.814889	825.087238	12.842061
14.000586	815.865849	12.847079
14.054232	816.772475	12.852096
14.032304	814.163702	12.857114
14.142811	807.704527	12.862131
14.227536	819.096779	12.867149
14.617305	822.842008	12.872167
14.400024	819.734513	12.877184
14.116701	810.949622	12.882202
14.864388	808.116837	12.887219
14.461311	822.564641	12.892237
14.429835	811.137335	12.897255
14.319225	810.202063	12.902272
14.268476	814.419421	12.907290
14.506109	802.744341	12.912307
14.646155	815.962638	12.917325
14.389233	810.874763	12.922343
14.140719	803.735194	12.927360
14.055265	814.445561	12.932378
14.533984	828.871053	12.937395
14.655519	849.561431	12.942413
14.503191	841.659826	12.947431
14.919582	849.249559	12.952448
14.439333	840.432934	12.957466
14.449163	815.544199	12.962483
14.563921	827.683816	12.967501
14.872395	831.958133	12.972519
14.720108	810.117686	12.977536
14.641238	818.187204	12.982554
14.776504	811.375870	12.987571
14.149688	802.147152	12.992589
14.374284	824.417804	12.997607
14.708951	830.632018	13.002624
14.837633	833.316760	13.007642
15.113102	838.956420	13.012659
14.762126	835.545977	13.017677
14.668796	819.911359	13.022695
14.502104	832.655949	13.027712
14.855914	836.660817	13.032730
14.922375	827.401359	13.037747
15.042442	830.220866	13.042765
14.992349	806.650369	13.047783
14.780773	815.632004	13.052800
14.722280	820.897398	13.057818
14.771629	802.956178	13.062835
14.098686	822.468014	13.067853
14.223976	831.249430	13.072871
14.882016	826.129324	13.077888
14.888302	842.812122	13.082906
14.702521	835.199068	13.087923
14.604045	839.002744	13.092941
14.980618	849.188048	13.097959
15.086410	840.622545	13.102976
14.890388	845.015957	13.107994
15.128572	841.119445	13.113011
15.056949	843.790251	13.118029
14.852269	835.305481	13.123047
14.627514	837.938513	13.128064
14.921093	837.189746	13.133082
15.055315	838.340392	13.138099
15.001277	850.571492	13.143117
14.869047	849.856384	13.148135
15.101500	833.909301	13.153152
14.599315	844.453361	13.158170
15.260796	853.419656	13.163187
15.502045	868.644427	13.168205
15.211860	856.538022	13.173223
15.426002	848.877275	13.178240
15.074613	835.885398	13.183258
15.218903	832.785165	13.188275
15.193805	841.358215	13.193293
15.306390	840.204791	13.198311
15.122409	838.953061	13.203328
15.218264	844.168158	13.208346
15.418959	839.338349	13.213363
15.656156	847.783033	13.218381
15.407312	839.226243	13.223399
15.183671	831.878356	13.228416
15.131537	844.892456	13.233434
15.378228	836.719441	13.238451
15.329082	841.060535	13.243469
15.253025	841.198289	13.248487
15.477009	843.187881	13.253504
15.301310	830.822661	13.258522
15.348524	839.083618	13.263539
15.504560	840.356326	13.268557
15.348012	833.423354	13.273575
15.255762	838.160770	13.278592
15.300727	841.056851	13.283610
15.478946	842.052813	13.288627
15.421509	844.122960	13.293645
15.458109	856.981685	13.298663
15.716672	856.179757	13.303680
15.347253	856.627851	13.308698
15.450945	853.319107	13.313715
15.624117	864.672570	13.318733
15.383540	864.324515	13.323751
15.183018	855.759238	13.328768
15.529777	869.012503	13.333786
15.620136	868.360691	13.338803
15.668424	863.830321	13.343821
15.883473	869.149820	13.348839
15.539853	861.609777	13.353856
15.362258	871.734634	13.358874
15.703245	871.884657	13.363891
15.855313	867.049295	13.368909
15.451010	867.242080	13.373927
16.088817	870.137227	13.378944
15.855342	872.424131	13.383962
15.959982	866.561658	13.388979
15.988174	869.831216	13.393997
15.782385	868.926627	13.399015
16.195265	862.541158	13.404032
15.778029	860.958059	13.409050
15.714123	865.491820	13.414067
15.673430	861.171887	13.419085
15.503589	867.044959	13.424103
15.698666	863.389971	13.429120
15.338892	875.542603	13.434138
15.873773	860.541298	13.439155
15.857968	861.094509	13.444173
15.435057	864.921497	13.449191
15.755486	861.291652	13.454208
16.002882	860.344647	13.459226
15.903373	872.731579	13.464243
15.869986	885.569615	13.469261
15.768422	882.889165	13.474279
16.322781	881.439152	13.479296
15.816510	894.820415	13.484314
16.298439	888.282606	13.489331
16.432505	891.424358	13.494349
16.579782	877.262146	13.499367
16.488030	866.729440	13.504384
16.021675	862.215528	13.509402
15.901562	867.063836	13.514419
16.243267	857.355800	13.519437
16.012249	859.587779	13.524455
16.356872	863.800433	13.529472
16.044164	865.084375	13.534490
16.067945	853.505609	13.539507
16.448560	861.080496	13.544525
16.103646	861.718699	13.549543
16.305129	848.838854	13.554560
16.377960	856.562713	13.559578
16.204704	860.590032	13.564595
16.179414	846.328830	13.569613
16.178512	855.882354	13.574631
16.159278	857.006303	13.579648
16.029459	854.710082	13.584666
16.465589	874.343572	13.589683
16.503379	883.006529	13.594701
16.144229	888.468651	13.599719
16.561647	886.532404	13.604736
16.457022	887.053354	13.609754
16.826249	884.928551	13.614771
16.832734	868.775609	13.619789
16.557759	863.126334	13.624807
16.825230	848.830625	13.629824
16.570330	856.942932	13.634842
16.167423	848.319585	13.639859
16.158376	847.725237	13.644877
16.284127	857.245334	13.649895
16.448564	851.373280	13.654912
16.534726	857.240159	13.659930
16.672495	874.550161	13.664947
17.172285	874.126009	13.669965
16.700160	867.984703	13.674983
16.656446	852.928949	13.680000
16.687989	841.712130	13.685018
16.548054	851.872771	13.690035
16.904983	847.489298	13.695053
16.871755	862.957417	13.700071
16.822593	852.010868	13.705088
16.554625	853.289286	13.710106
16.583294	845.150130	13.715123
16.625871	853.420029	13.720141
16.854727	850.421643	13.725159
16.914275	848.446920	13.730176
16.510386	846.574367	13.735194
16.557342	859.851187	13.740211
17.096535	861.130054	13.745229
17.180686	868.291029	13.750247
16.802175	848.220863	13.755264
16.731953	854.828413	13.760282
16.665112	863.331615	13.765299
17.058214	872.561326	13.770317
16.862353	880.855094	13.775335
17.059466	884.326029	13.780352
17.267672	888.532597	13.785370
16.900665	857.889898	13.790387
16.884429	857.981258	13.795405
16.717769	877.054347	13.800423
17.021060	881.053305	13.805440
17.150216	886.214103	13.810458
17.179635	889.858001	13.815475
17.359736	881.783943	13.820493
17.191605	889.528055	13.825511
17.116305	865.871983	13.830528
16.644991	864.880490	13.835546
16.983086	878.347656	13.840563
17.161794	878.605189	13.845581
16.944496	870.094734	13.850599
16.725473	882.700206	13.855616
16.951110	893.192911	13.860634
16.959066	887.729310	13.865651
17.126082	881.936922	13.870669
16.845451	885.175544	13.875687
16.906201	886.962435	13.880704
16.955101	888.999959	13.885722
16.671200	914.099943	13.890739
17.220744	910.063197	13.895757
17.259296	912.149277	13.900775
17.241145	913.546230	13.905792
17.485520	914.150132	13.910810
17.082501	910.478636	13.915827
17.403387	909.989282	13.920845
17.212343	913.055259	13.925863
17.412847	904.372415	13.930880
17.862668	911.879109	13.935898
17.462198	906.256855	13.940915
17.389936	907.183801	13.945933
17.301179	923.852970	13.950951
17.423694	915.469766	13.955968
17.545953	908.910887	13.960986
17.127817	906.772914	13.966003
17.708050	898.981382	13.971021
17.688150	911.960296	13.976039
17.633301	905.322930	13.981056
17.814628	902.889769	13.986074
17.399254	916.500867	13.991091
17.695643	905.919345	13.996109
17.404453	903.623509	14.001127
17.467984	910.287804	14.006144
17.817590	926.731315	14.011162
18.060255	931.362340	14.016179
18.350950	908.357307	14.021197
17.961715	912.187007	14.026215
18.153182	906.830352	14.031232
18.297308	892.021323	14.036250
18.216164	901.938958	14.041267
18.062295	907.371788	14.046285
17.971820	896.817791	14.051303
17.830670	898.290670	14.056320
17.900411	893.791779	14.061338
17.629358	899.423466	14.066355
18.039202	893.179111	14.071373
18.064393	897.647281	14.076391
17.710401	902.306928	14.081408
18.125959	898.888282	14.086426
17.920912	898.768958	14.091443
18.483318	902.043434	14.096461
17.922736	889.568966	14.101479
18.166554	880.013583	14.106496
18.022270	883.523419	14.111514
17.606676	881.199826	14.116531
18.216187	877.854921	14.121549
17.790836	900.999585	14.126567
18.333966	907.484150	14.131584
18.061232	900.029501	14.136602
18.115254	903.718540	14.141619
18.174461	897.316516	14.146637
18.180650	895.487981	14.151655
18.455281	906.869681	14.156672
18.203206	905.276899	14.161690
17.950340	902.967940	14.166707
18.219141	904.044392	14.171725
18.407975	899.805788	14.176743
18.377144	895.054963	14.181760
18.137178	892.817679	14.186778
18.262063	903.014499	14.191795
18.042120	896.596609	14.196813
18.051290	897.429108	14.201831
18.174297	901.378941	14.206848
18.341607	890.359493	14.211866
18.338487	894.978869	14.216883
18.247043	902.320326	14.221901
18.255017	895.714012	14.226919
18.286657	896.790785	14.231936
18.301896	885.236237	14.236954
18.151191	906.290716	14.241971
18.580675	906.494508	14.246989
18.501146	918.589841	14.252007
18.292470	917.588794	14.257024
18.613092	924.521185	14.262042
18.487234	929.617563	14.267059
18.623860	922.663363	14.272077
18.351915	926.135851	14.277095
18.531276	936.887762	14.282112
19.014525	918.472414	14.287130
18.707786	938.137424	14.292147
18.856976	925.703776	14.297165
18.621353	936.821751	14.302183
18.809950	926.564273	14.307200
19.005434	922.618114	14.312218
18.705208	936.722019	14.317235
18.921046	922.669182	14.322253
18.976030	904.644446	14.327271
18.712618	902.842552	14.332288
18.631186	902.032154	14.337306
18.732720	911.086095	14.342323
18.836842	921.482976	14.347341
18.955397	919.580171	14.352359
18.716973	915.483514	14.357376
19.053160	924.512266	14.362394
18.881025	933.854906	14.367411
19.007821	924.569281	14.372429
18.848190	923.739132	14.377447
18.757235	931.457424	14.382464
19.080317	928.282359	14.387482
18.565886	923.552199	14.392499
18.739448	922.676830	14.397517
19.022410	931.645498	14.402535
18.941260	924.665780	14.407552
19.160049	926.877265	14.412570
18.953575	929.397469	14.417587
19.212409	927.234811	14.422605
19.053056	922.155869	14.427623
18.975414	924.374713	14.432640
19.233545	930.773732	14.437658
19.284080	927.624910	14.442675
19.155835	921.984136	14.447693
19.128607	923.575961	14.452711
19.127422	936.269078	14.457728
19.314844	926.675357	14.462746
18.895985	933.760754	14.467763
19.128954	938.569336	14.472781
19.455839	949.731545	14.477799
19.235975	951.165575	14.482816
19.425183	952.741614	14.487834
19.371065	957.437436	14.492851
19.411748	957.093776	14.497869
19.344496	955.371842	14.502887
19.619839	954.195450	14.507904
19.689458	955.304822	14.512922
19.158468	938.339801	14.517939
19.778531	941.983923	14.522957
19.571426	947.850489	14.527975
19.542129	942.849145	14.532992
19.627777	924.137255	14.538010
19.471244	928.501630	14.543027
19.219594	922.114850	14.548045
19.612425	941.493325	14.553063
19.580030	945.013420	14.558080
19.386524	948.298670	14.563098
19.402788	943.485628	14.568115
19.219325	952.926886	14.573133
19.620865	948.105873	14.578151
19.411720	952.278788	14.583168
19.524682	940.189736	14.588186
19.478230	960.063980	14.593203
19.558014	951.355003	14.598221
19.550165	953.251547	14.603239
19.413032	974.314997	14.608256
19.786446	973.990749	14.613274
20.156152	970.831982	14.618291
19.973408	973.600195	14.623309
20.063340	973.917275	14.628327
20.026851	975.826132	14.633344
20.267003	970.552437	14.638362
19.753004	958.304426	14.643379
19.792130	948.357901	14.648397
20.241145	947.205852	14.653415
20.061059	956.472372	14.658432
19.821725	938.601137	14.663450
19.755421	948.681083	14.668467
20.029022	973.112268	14.673485
20.338987	965.891257	14.678503
20.085848	968.776792	14.683520
20.112873	973.495916	14.688538
20.222348	980.408904	14.693555
20.305070	977.296773	14.698573
20.503463	961.768794	14.703591
20.202410	947.934202	14.708608
20.111192	936.271541	14.713626
20.024399	939.275619	14.718643
20.208305	948.886932	14.723661
20.568602	951.692349	14.728679
20.028382	951.100651	14.733696
20.534650	945.502526	14.738714
20.459868	943.706064	14.743731
20.161408	945.241648	14.748749
20.403794	951.575671	14.753767
19.820984	956.183399	14.758784
20.459597	962.187823	14.763802
20.375027	967.087858	14.768819
20.087884	964.554968	14.773837
20.523747	966.424539	14.778855
20.540965	973.085789	14.783872
20.638058	953.781623	14.788890
20.455365	964.925117	14.793907
20.486794	969.511646	14.798925
20.482595	962.048706	14.803943
20.560223	966.177384	14.808960
20.561045	965.462130	14.813978
20.604294	977.020283	14.818995
20.365910	972.542174	14.824013
20.624799	965.355485	14.829031
20.420335	962.114271	14.834048
20.386052	970.090394	14.839066
20.659910	971.484365	14.844083
20.325612	962.406289	14.849101
20.745181	964.084590	14.854119
20.624792	983.700364	14.859136
21.056365	974.529177	14.864154
20.591689	978.615903	14.869171
20.735477	979.632916	14.874189
21.445126	979.132456	14.879207
21.483131	972.159891	14.884224
21.364762	952.190668	14.889242
21.464428	954.029984	14.894259
21.297987	957.772689	14.899277
21.460237	952.190868	14.904295
21.138030	938.027358	14.909312
20.861340	921.250212	14.914330
21.034880	916.742231	14.919347
20.884633	917.799662	14.924365
21.203188	917.024523	14.929383
21.175332	926.586678	14.934400
20.947060	913.803187	14.939418
20.976649	916.553227	14.944435
20.942791	942.226001	14.949453
21.212404	937.772696	14.954471
21.211525	959.571447	14.959488
21.155280	954.409424	14.964506
21.267008	953.602627	14.969523
21.013130	951.863511	14.974541
21.425052	955.242873	14.979559
21.485329	948.497994	14.984576
21.254630	955.818895	14.989594
21.401561	944.897935	14.994611
21.102716	951.957702	14.999629
21.317494	955.306760	15.004647
21.216369	954.506600	15.009664
21.466353	944.546784	15.014682
21.047663	956.948642	15.019699
21.160339	956.778879	15.024717
21.275710	944.551359	15.029735
21.271685	947.831080	15.034752
21.138780	947.015801	15.039770
21.297337	941.445714	15.044787
21.247225	954.424934	15.049805
21.369857	948.420406	15.054823
21.444156	960.622710	15.059840
21.373000	963.381141	15.064858
21.458388	978.079808	15.069875
21.593563	992.148323	15.074893
21.803656	970.857007	15.079911
21.625147	974.701792	15.084928
21.689295	976.128155	15.089946
21.704347	968.524949	15.094963
21.575235	985.567226	15.099981
22.064690	972.433919	15.104999
21.758041	973.134491	15.110016
21.514223	976.727320	15.115034
21.234328	986.177448	15.120051
21.553753	978.980256	15.125069
21.624720	974.699703	15.130087
21.710332	977.577481	15.135104
21.803693	975.093207	15.140122
21.905656	985.254407	15.145139
21.866074	1003.651847	15.150157
22.182219	994.727636	15.155175
22.196200	1000.390984	15.160192
22.463095	975.815451	15.165210
22.170250	972.825905	15.170227
21.836946	978.025761	15.175245
22.053497	971.193642	15.180263
22.157509	971.233739	15.185280
22.220752	975.466058	15.190298
22.180205	970.921306	15.195315
21.824937	969.367810	15.200333
22.025636	965.500391	15.205351
22.201356	971.407917	15.210368
21.803395	975.367496	15.215386
22.420263	984.504993	15.220403
22.340427	992.916336	15.225421
22.542985	994.526387	15.230439
22.220352	977.497270	15.235456
21.834128	978.665046	15.240474
21.986270	981.700797	15.245491
22.241232	1008.856886	15.250509
22.448022	999.430066	15.255527
22.428960	994.072056	15.260544
22.199927	1014.975778	15.265562
22.225804	1012.344705	15.270579
22.190836	1010.672341	15.275597
22.177801	1003.359143	15.280615
22.213861	1002.844622	15.285632
22.413949	1005.165589	15.290650
22.311115	1001.054178	15.295667
22.504227	1016.018987	15.300685
22.758498	1017.908044	15.305703
23.107221	1031.079938	15.310720
22.650447	1017.125273	15.315738
23.012038	991.979929	15.320755
22.785251	1010.436655	15.325773
22.720244	999.569771	15.330791
23.051425	990.037868	15.335808
22.806652	989.969785	15.340826
23.052392	992.503639	15.345843
22.716197	996.340537	15.350861
22.927792	992.870944	15.355879
23.154719	994.563076	15.360896
22.632386	989.027944	15.365914
22.983841	990.882929	15.370931
22.862009	993.065393	15.375949
22.762906	995.580263	15.380967
23.125745	1000.922819	15.385984
23.111713	987.624319	15.391002
23.062703	987.608812	15.396019
22.784873	1000.943658	15.401037
22.830593	988.185090	15.406055
23.001267	988.820561	15.411072
22.967703	996.822755	15.416090
22.853790	997.693411	15.421107
22.810234	997.707805	15.426125
23.156491	1006.163880	15.431143
23.257647	1024.247193	15.436160
23.362901	1020.013511	15.441178
23.375881	1004.865380	15.446195
22.975259	1003.442090	15.451213
23.211073	1006.661031	15.456231
23.070634	1013.271199	15.461248
23.238429	1028.955730	15.466266
23.563720	1022.287871	15.471283
23.398972	1010.065061	15.476301
23.778757	1019.878458	15.481319
23.296196	1013.730747	15.486336
23.367707	1024.575629	15.491354
23.739494	1017.479098	15.496371
23.421706	1009.692627	15.501389
23.258120	1007.990346	15.506407
23.461104	997.792045	15.511424
23.049649	1021.555450	15.516442
23.470716	1022.727398	15.521459
23.503207	1026.025998	15.526477
23.838133	1015.127358	15.531495
23.398726	1017.441228	15.536512
23.391676	1031.524229	15.541530
23.845349	1020.298928	15.546547
23.287641	1017.001235	15.551565
23.571563	1023.410398	15.556583
23.489244	1015.965852	15.561600
23.426364	1017.345900	15.566618
23.412120	1015.853642	15.571635
23.341714	1023.373932	15.576653
24.045547	1034.731053	15.581671
23.988194	1055.172086	15.586688
24.153238	1049.187671	15.591706
24.110859	1024.132157	15.596723
23.713685	1011.739719	15.601741
23.696962	1017.511476	15.606759
24.149919	1014.390608	15.611776
24.100668	1044.565811	15.616794
24.129362	1030.010526	15.621811
23.879498	1018.036577	15.626829
23.981553	1027.263208	15.631847
24.085590	1035.081392	15.636864
24.186955	1050.617600	15.641882
24.248587	1040.225640	15.646899
24.004580	1022.567935	15.651917
23.982157	1029.319997	15.656935
24.400871	1045.226519	15.661952
24.317475	1061.742124	15.666970
24.327975	1039.504728	15.671987
24.241484	1038.859992	15.677005
24.204378	1040.584247	15.682023
24.649869	1048.457607	15.687040
24.365419	1039.441904	15.692058
24.458120	1019.777124	15.697075
24.319294	1013.734098	15.702093
24.115506	1011.855125	15.707111
24.473784	1023.793168	15.712128
24.502811	1039.515993	15.717146
24.419324	1041.495901	15.722163
24.277823	1043.493269	15.727181
24.639520	1040.840942	15.732199
24.667757	1033.997008	15.737216
23.765936	1053.491259	15.742234
24.728725	1043.962805	15.747251
24.584190	1037.796915	15.752269
24.457672	1042.930049	15.757287
24.608236	1040.225619	15.762304
24.225190	1048.532696	15.767322
24.463358	1040.212975	15.772339
24.440265	1049.097469	15.777357
24.421248	1050.689426	15.782375
24.697580	1049.779650	15.787392
24.759534	1059.954203	15.792410
24.992357	1061.967065	15.797427
24.998717	1065.780830	15.802445
24.954402	1071.410932	15.807463
25.024250	1052.399776	15.812480
24.778491	1064.826186	15.817498
25.270444	1068.816356	15.822515
25.293146	1047.710401	15.827533
24.823617	1052.913211	15.832551
24.646400	1046.500990	15.837568
24.777599	1040.280874	15.842586
25.210387	1051.135352	15.847603
25.527202	1056.517024	15.852621
25.121443	1049.951263	15.857639
25.443646	1033.452126	15.862656
24.901030	1042.847001	15.867674
24.579232	1045.281378	15.872691
24.845893	1047.541555	15.877709
25.003113	1062.184444	15.882727
25.315230	1049.484934	15.887744
25.070591	1061.808811	15.892762
25.048505	1056.088152	15.897779
25.113906	1050.673848	15.902797
25.146235	1057.246825	15.907815
25.126164	1050.227433	15.912832
25.054437	1060.866129	15.917850
25.781323	1065.377223	15.922867
25.805144	1057.726665	15.927885
25.415260	1061.238846	15.932903
25.431321	1051.948907	15.937920
25.639638	1054.090009	15.942938
25.539611	1051.781848	15.947955
25.449567	1054.285193	15.952973
25.415573	1056.877094	15.957991
25.834251	1060.403862	15.963008
25.754198	1054.307808	15.968026
25.449311	1044.993365	15.973043
25.759884	1054.729457	15.978061
25.760558	1062.212828	15.983079
25.832706	1046.416699	15.988096
25.950724	1050.120095	15.993114
25.749721	1060.446155	15.998131
25.773265	1046.518174	16.003149
25.716687	1055.575499	16.008167
25.889081	1073.067767	16.013184
25.969285	1069.947276	16.018202
26.068117	1077.838771	16.023219
25.962189	1058.473255	16.028237
25.755521	1062.549153	16.033255
25.843429	1060.994644	16.038272
25.626989	1080.833465	16.043290
26.067643	1083.600632	16.048307
26.186718	1079.322925	16.053325
25.968744	1090.322759	16.058343
26.122156	1078.359962	16.063360
26.155171	1080.863051	16.068378
26.309153	1074.098106	16.073395
26.557355	1068.921456	16.078413
26.062270	1077.113031	16.083431
26.243203	1065.878643	16.088448
26.598942	1070.185959	16.093466
26.382529	1082.009012	16.098483
26.256466	1078.796445	16.103501
26.050122	1071.694655	16.108519
26.347306	1072.849979	16.113536
26.286406	1070.592230	16.118554
26.203044	1072.860065	16.123571
26.307148	1085.523901	16.128589
26.460776	1078.496458	16.133607
26.603379	1064.569649	16.138624
26.419680	1076.270185	16.143642
26.371723	1078.645931	16.148659
26.827020	1066.086695	16.153677
26.503326	1079.522086	16.158695
26.453440	1074.452558	16.163712
26.436272	1073.561365	16.168730
26.471141	1074.692528	16.173747
26.314977	1070.353042	16.178765
26.562152	1094.804829	16.183783
27.184848	1096.413168	16.188800
27.117778	1097.442301	16.193818
26.800262	1088.914432	16.198835
26.963556	1074.580129	16.203853
27.075640	1066.860069	16.208871
27.000324	1055.021687	16.213888
26.973258	1058.600858	16.218906
26.766356	1065.423572	16.223923
26.900481	1056.844705	16.228941
26.908251	1067.613551	16.233959
27.223939	1059.714401	16.238976
26.683793	1077.003610	16.243994
26.343989	1073.537831	16.249011
26.832236	1075.811190	16.254029
26.710847	1097.256886	16.259047
26.900760	1098.894231	16.264064
27.173202	1090.166919	16.269082
27.280174	1101.197498	16.274099
27.418108	1087.327926	16.279117
27.290093	1096.640740	16.284135
27.202288	1091.922690	16.289152
27.314507	1096.279308	16.294170
27.231854	1093.485280	16.299187
27.467652	1095.461244	16.304205
27.096781	1099.347984	16.309223
27.009176	1099.750891	16.314240
27.445602	1099.677897	16.319258
26.981848	1096.760263	16.324275
27.655292	1107.768878	16.329293
27.798358	1103.828088	16.334311
27.565205	1094.757426	16.339328
27.503448	1094.115292	16.344346
27.301118	1097.677970	16.349363
27.764355	1101.963004	16.354381
27.619341	1120.923290	16.359399
27.640787	1113.681296	16.364416
27.887923	1114.749831	16.369434
27.833795	1123.283846	16.374451
27.868121	1104.662094	16.379469
27.874398	1093.928122	16.384487
27.962479	1092.111224	16.389504
28.137829	1081.203873	16.394522
27.531751	1083.545493	16.399539
27.734771	1081.753295	16.404557
28.112140	1103.535013	16.409575
27.897478	1087.819892	16.414592
27.992647	1073.988497	16.419610
27.771723	1095.036732	16.424627
28.152840	1110.023312	16.429645
27.978621	1113.419367	16.434663
27.957461	1107.093321	16.439680
28.036819	1116.738549	16.444698
27.768888	1120.645088	16.449715
27.942459	1114.028832	16.454733
28.231406	1127.509654	16.459751
28.189969	1117.293112	16.464768
28.292437	1115.212657	16.469786
27.907865	1118.802109	16.474803
28.207367	1107.996054	16.479821
28.287207	1117.391245	16.484839
28.111084	1112.824964	16.489856
28.435596	1114.527849	16.494874
28.058869	1122.819357	16.499891
28.268339	1125.132297	16.504909
28.494187	1119.218305	16.509927
28.453860	1126.142041	16.514944
28.870909	1130.392400	16.519962
28.215249	1127.943408	16.524979
28.677494	1123.367681	16.529997
28.671679	1135.898567	16.535015
28.721599	1137.831249	16.540032
28.697895	1118.291860	16.545050
28.413092	1131.332548	16.550067
28.783694	1127.802305	16.555085
28.725173	1128.956385	16.560103
28.613902	1137.142036	16.565120
29.090419	1142.843550	16.570138
28.868150	1130.039794	16.575155
28.999800	1119.950331	16.580173
28.683355	1117.132542	16.585191
28.803051	1126.589644	16.590208
29.186604	1125.767049	16.595226
28.957417	1121.849586	16.600243
28.999960	1108.164629	16.605261
28.849088	1112.710373	16.610279
29.090324	1125.113038	16.615296
29.129136	1130.478482	16.620314
29.182973	1137.802342	16.625331
29.354826	1117.998393	16.630349
28.977556	1105.736721	16.635367
29.119681	1116.302326	16.640384
29.432023	1124.324480	16.645402
29.065055	1125.004421	16.650419
29.250521	1122.218434	16.655437
29.100667	1126.656552	16.660455
29.356190	1129.534622	16.665472
29.494713	1124.823445	16.670490
29.368054	1127.452911	16.675507
29.218720	1129.030591	16.680525
29.288703	1124.331921	16.685543
29.201760	1126.759187	16.690560
29.196785	1120.153145	16.695578
28.983150	1129.358101	16.700595
29.297798	1119.850500	16.705613
29.216090	1122.003127	16.710631
29.257188	1146.873240	16.715648
29.623665	1146.563815	16.720666
29.863939	1155.959875	16.725683
29.899550	1152.777456	16.730701
29.750877	1156.542466	16.735719
29.789042	1155.392362	16.740736
30.123221	1141.177962	16.745754
29.755309	1132.915834	16.750771
29.598125	1125.013901	16.755789
29.595297	1146.417439	16.760807
29.547854	1145.301755	16.765824
29.986962	1153.137058	16.770842
30.147895	1156.580872	16.775859
30.078932	1154.414388	16.780877
29.922766	1148.957150	16.785895
29.912481	1149.280560	16.790912
29.968747	1148.616952	16.795930
30.007481	1157.768805	16.800947
29.979004	1154.712311	16.805965
29.993696	1153.239565	16.810983
29.842859	1145.130504	16.816000
30.252790	1146.294166	16.821018
29.886549	1158.150894	16.826035
29.823284	1154.688405	16.831053
30.171490	1164.679330	16.836071
30.169684	1184.533793	16.841088
30.491425	1173.694494	16.846106
30.463188	1171.709831	16.851123
30.579833	1177.497988	16.856141
30.382832	1182.551098	16.861159
30.433407	1175.996078	16.866176
30.778351	1174.660654	16.871194
30.822582	1169.424188	16.876211
30.595791	1174.313938	16.881229
30.848647	1171.984250	16.886247
30.978222	1164.722199	16.891264
30.730566	1143.805057	16.896282
30.616146	1147.349085	16.901299
30.551948	1146.097807	16.906317
30.874665	1136.810479	16.911335
30.565391	1144.017407	16.916352
30.855750	1136.862833	16.921370
30.544979	1140.755593	16.926387
30.815740	1152.289764	16.931405
31.208700	1172.471629	16.936423
31.029624	1156.266187	16.941440
31.348237	1146.339283	16.946458
30.977339	1145.788580	16.951475
30.948462	1134.405379	16.956493
30.873033	1149.214335	16.961511
30.562012	1150.454622	16.966528
31.288469	1144.803704	16.971546
31.258594	1171.140661	16.976563
31.366187	1170.706917	16.981581
31.212174	1148.747098	16.986599
30.757352	1146.475116	16.991616
31.197886	1162.203971	16.996634
31.276644	1171.645626	17.001651
31.353303	1163.371620	17.006669
31.209432	1174.693270	17.011687
31.334781	1180.055453	17.016704
31.347208	1164.149996	17.021722
31.335966	1180.117868	17.026739
31.315960	1180.974689	17.031757
31.513902	1170.932890	17.036775
31.491188	1166.321561	17.041792
31.329537	1167.257684	17.046810
31.244152	1177.531454	17.051827
31.304789	1164.505160	17.056845
31.297316	1171.572282	17.061863
31.299045	1194.525866	17.066880
31.773357	1194.009872	17.071898
31.922962	1193.245221	17.076915
32.005022	1189.868535	17.081933
32.288279	1194.275448	17.086951
31.928507	1173.035902	17.091968
31.844725	1162.378763	17.096986
31.729909	1161.418479	17.102003
31.515841	1160.746205	17.107021
31.828456	1177.614733	17.112039
32.016682	1196.011465	17.117056
32.001129	1186.133064	17.122074
32.033897	1201.295587	17.127091
31.993801	1194.947048	17.132109
32.313008	1186.516825	17.137127
32.568137	1184.575673	17.142144
32.255882	1191.188920	17.147162
32.307158	1188.676434	17.152179
32.112487	1185.092960	17.157197
32.233302	1186.797630	17.162215
32.330022	1188.324617	17.167232
32.414446	1188.065343	17.172250
32.157956	1192.012916	17.177267
32.095148	1184.029029	17.182285
32.597458	1184.481479	17.187303
32.237543	1199.505971	17.192320
32.277684	1188.183163	17.197338
32.191940	1195.332117	17.202355
32.211310	1186.771550	17.207373
32.190912	1182.479664	17.212391
32.231756	1196.570352	17.217408
32.441921	1208.524946	17.222426
33.134455	1208.506859	17.227443
33.134747	1211.944559	17.232461
33.052389	1204.232746	17.237479
32.613717	1194.551602	17.242496
32.357226	1182.709996	17.247514
32.815944	1196.414555	17.252531
32.758853	1210.712551	17.257549
32.988720	1198.398498	17.262567
32.677598	1219.245505	17.267584
33.122640	1213.478100	17.272602
33.110917	1199.550494	17.277619
33.171214	1204.105063	17.282637
33.351264	1203.630216	17.287655
32.914281	1188.518568	17.292672
32.894242	1201.067801	17.297690
33.514364	1213.627970	17.302707
33.031186	1208.533754	17.307725
33.539741	1202.717085	17.312743
33.535795	1199.177472	17.317760
33.204362	1175.989654	17.322778
33.128754	1185.804212	17.327795
32.839440	1179.510049	17.332813
33.127443	1193.795483	17.337831
33.188611	1204.049384	17.342848
33.560661	1210.621987	17.347866
33.366227	1199.020466	17.352883
33.128097	1205.613795	17.357901
33.654983	1202.170290	17.362919
33.091866	1201.755466	17.367936
33.416698	1208.092997	17.372954
33.278706	1200.933402	17.377971
33.389997	1202.554621	17.382989
33.497775	1225.131533	17.388007
33.460192	1230.447638	17.393024
33.554260	1222.434855	17.398042
34.059450	1224.112619	17.403059
34.184813	1238.229530	17.408077
34.268263	1224.453470	17.413095
34.057596	1226.598686	17.418112
33.921494	1226.146363	17.423130
34.041208	1223.140355	17.428147
34.017543	1223.798209	17.433165
34.237092	1218.347745	17.438183
33.989386	1226.686677	17.443200
33.764161	1221.222324	17.448218
33.950346	1228.839070	17.453235
33.820639	1232.733817	17.458253
34.483885	1218.082942	17.463271
33.957612	1232.820047	17.468288
34.003125	1233.298189	17.473306
34.027803	1227.222745	17.478323
33.936732	1227.287897	17.483341
34.012064	1230.118216	17.488359
34.357662	1238.649813	17.493376
34.537038	1249.087524	17.498394
34.397996	1248.622893	17.503411
34.561975	1249.529813	17.508429
34.691639	1241.179891	17.513447
34.554535	1250.220721	17.518464
34.619148	1241.696538	17.523482
34.772914	1249.465479	17.528499
34.406036	1258.125845	17.533517
34.738378	1247.027304	17.538535
34.466528	1259.408583	17.543552
34.511744	1253.477153	17.548570
34.672663	1254.396191	17.553587
34.409794	1251.416201	17.558605
34.673087	1253.220542	17.563623
34.897921	1255.393977	17.568640
34.612014	1251.430941	17.573658
35.041153	1238.023661	17.578675
34.579016	1247.457911	17.583693
34.807947	1261.450068	17.588711
34.937701	1271.945593	17.593728
35.147099	1281.238779	17.598746
35.415428	1284.186602	17.603763
35.036162	1273.969885	17.608781
35.541643	1274.097258	17.613799
35.677756	1278.944982	17.618816
35.452210	1252.750253	17.623834
35.565033	1235.303766	17.628851
35.477171	1239.756865	17.633869
35.456855	1234.223218	17.638887
35.231451	1237.002464	17.643904
35.368055	1237.279559	17.648922
35.501600	1233.258235	17.653939
35.470968	1247.181872	17.658957
35.259286	1240.815219	17.663975
35.203500	1244.361980	17.668992
35.476479	1265.785649	17.674010
35.788073	1273.206328	17.679027
35.294157	1271.450549	17.684045
35.198078	1260.281675	17.689063
35.422285	1271.701601	17.694080
35.192278	1269.173389	17.699098
35.458639	1276.219123	17.704115
35.608001	1295.607282	17.709133
35.893883	1287.752896	17.714151
36.357815	1293.412066	17.719168
36.158189	1295.094712	17.724186
36.156341	1283.272356	17.729203
36.155249	1292.794396	17.734221
36.565742	1294.086501	17.739239
36.381715	1274.208897	17.744256
36.185094	1254.271598	17.749274
36.189728	1249.693907	17.754291
36.216027	1266.205186	17.759309
36.480963	1265.364593	17.764327
36.401274	1255.839999	17.769344
36.152351	1258.522167	17.774362
36.299277	1256.718553	17.779379
36.198549	1265.511883	17.784397
36.390083	1275.555342	17.789415
36.534220	1277.976921	17.794432
36.481528	1284.970478	17.799450
36.455947	1290.284030	17.804467
36.743492	1289.322592	17.809485
36.741431	1289.147479	17.814503
36.914199	1290.779806	17.819520
36.731958	1279.199631	17.824538
36.839046	1253.855893	17.829555
36.706580	1259.216620	17.834573
36.814848	1268.611340	17.839591
36.726038	1266.844121	17.844608
36.582685	1286.147787	17.849626
36.659187	1277.477154	17.854643
36.525301	1285.307819	17.859661
36.487919	1290.955553	17.864679
36.498850	1282.898808	17.869696
36.579511	1274.785670	17.874714
37.268251	1297.450121	17.879731
36.912049	1304.919957	17.884749
37.078263	1307.549868	17.889767
37.424746	1316.505510	17.894784
37.163817	1312.971335	17.899802
37.334580	1312.536399	17.904819
37.556879	1311.857747	17.909837
37.465495	1298.836581	17.914855
37.129654	1291.248490	17.919872
36.782207	1315.121830	17.924890
37.513010	1311.062213	17.929907
37.301709	1310.812442	17.934925
37.000152	1318.113043	17.939943
37.459327	1312.481434	17.944960
37.331778	1306.083924	17.949978
37.644904	1313.420327	17.954995
37.702810	1316.497205	17.960013
37.155242	1313.399904	17.965031
37.306524	1309.622639	17.970048
37.546662	1333.756138	17.975066
37.810052	1333.825305	17.980083
38.097398	1335.561911	17.985101
38.242680	1337.207641	17.990119
38.496101	1318.726366	17.995136
38.152902	1317.178907	18.000154
38.213799	1305.355416	18.005171
38.066243	1306.141406	18.010189
38.204035	1309.407413	18.015207
38.175503	1305.474262	18.020224
37.842707	1310.496121	18.025242
38.253613	1296.493471	18.030259
37.997903	1300.522622	18.035277
38.072537	1298.670722	18.040295
38.204118	1297.150895	18.045312
38.081687	1300.224505	18.050330
38.051593	1308.548778	18.055347
38.463763	1319.110051	18.060365
38.453533	1330.036363	18.065383
38.043374	1324.825333	18.070400
38.322414	1327.822764	18.075418
38.524646	1319.107515	18.080435
38.661148	1323.531042	18.085453
38.608590	1325.693051	18.090471
38.674871	1318.155014	18.095488
38.570214	1322.053517	18.100506
38.723823	1333.573922	18.105523
39.085823	1323.330726	18.110541
38.496648	1321.376345	18.115559
38.626974	1328.616801	18.120576
38.668505	1326.517061	18.125594
38.581784	1330.833995	18.130611
38.978543	1342.096936	18.135629
38.680355	1365.343804	18.140647
39.046223	1355.780357	18.145664
39.004102	1366.374417	18.150682
39.150945	1359.277112	18.155699
39.352268	1363.266971	18.160717
39.261656	1359.442868	18.165735
39.496699	1365.458936	18.170752
39.659366	1358.154323	18.175770
39.562148	1342.803530	18.180787
39.474555	1327.546029	18.185805
39.491837	1322.309240	18.190823
39.227347	1318.422753	18.195840
39.299597	1331.510300	18.200858
39.486762	1340.202958	18.205875
39.409794	1354.626794	18.210893
39.515884	1355.680274	18.215911
39.880642	1353.383635	18.220928
39.445070	1359.715409	18.225946
39.569631	1358.782868	18.230963
39.552186	1346.505826	18.235981
39.561152	1360.407670	18.240999
39.563050	1355.989235	18.246016
39.228026	1357.045540	18.251034
39.404894	1355.180283	18.256051
39.512757	1359.929173	18.261069
39.551530	1364.718217	18.266087
39.792878	1371.551823	18.271104
39.710434	1376.406368	18.276122
39.748463	1362.066713	18.281139
39.882757	1375.578625	18.286157
39.826379	1373.478918	18.291175
39.964424	1369.344037	18.296192
39.901904	1384.527802	18.301210
40.614307	1395.446146	18.306227
40.945259	1395.242770	18.311245
40.785571	1376.763165	18.316263
40.721226	1360.574762	18.321280
40.393259	1369.438178	18.326298
40.666470	1366.756725	18.331315
40.794090	1361.670759	18.336333
40.731073	1368.194478	18.341351
40.648928	1358.239385	18.346368
40.372963	1364.400320	18.351386
40.741902	1360.556174	18.356403
40.634789	1364.664117	18.361421
40.295079	1371.221947	18.366439
40.624350	1359.529630	18.371456
40.638433	1358.341765	18.376474
40.495347	1362.400542	18.381491
40.590910	1366.645244	18.386509
41.014142	1377.204335	18.391527
41.141019	1385.206298	18.396544
41.035677	1396.839807	18.401562
40.848832	1396.217740	18.406579
41.140088	1391.718215	18.411597
41.009092	1394.686582	18.416615
41.122782	1388.533186	18.421632
40.801273	1391.279726	18.426650
40.851065	1381.448857	18.431667
41.129538	1388.341680	18.436685
40.826636	1390.652532	18.441703
41.471303	1408.818014	18.446720
41.397704	1417.815973	18.451738
41.722489	1406.063544	18.456755
41.718246	1402.495394	18.461773
41.697795	1407.054707	18.466791
42.071281	1392.496818	18.471808
41.827094	1377.622965	18.476826
41.662973	1373.833247	18.481843
41.830265	1369.093426	18.486861
41.538898	1368.918489	18.491879
41.631187	1371.264018	18.496896
41.767477	1380.158974	18.501914
41.563033	1385.783964	18.506931
41.941191	1392.221799	18.511949
42.145211	1396.596399	18.516967
42.353254	1398.544908	18.521984
42.113726	1402.453122	18.527002
42.208621	1399.894423	18.532019
42.695957	1395.003099	18.537037
42.443550	1384.447872	18.542055
42.194038	1368.867532	18.547072
42.210545	1367.037433	18.552090
42.067779	1363.273318	18.557107
42.176894	1356.555815	18.562125
42.056792	1371.250338	18.567143
42.571194	1379.425429	18.572160
42.712741	1388.172889	18.577178
42.365340	1397.605197	18.582195
42.649801	1391.440507	18.587213
42.391865	1399.790474	18.592231
42.408015	1390.685327	18.597248
42.614618	1383.490944	18.602266
42.801076	1382.573957	18.607283
42.620419	1390.118550	18.612301
42.673513	1388.365461	18.617319
42.871631	1383.819134	18.622336
43.034921	1382.273589	18.627354
42.759512	1389.660047	18.632371
42.982463	1395.182529	18.637389
42.464952	1395.966478	18.642407
42.730848	1398.471681	18.647424
42.486845	1389.059184	18.652442
42.374800	1401.117363	18.657459
43.077838	1408.215980	18.662477
42.712606	1424.723832	18.667495
43.240792	1427.011312	18.672512
43.033433	1424.765904	18.677530
42.901772	1441.341656	18.682547
42.926715	1418.914146	18.687565
43.048367	1433.239890	18.692583
43.219121	1447.503407	18.697600
43.352933	1459.676297	18.702618
43.372557	1451.689277	18.707635
43.630404	1446.451861	18.712653
43.555513	1453.579459	18.717671
43.786260	1445.217052	18.722688
43.717887	1444.221914	18.727706
43.382422	1447.211680	18.732723
43.986681	1441.274791	18.737741
43.711868	1444.884167	18.742759
43.510933	1434.659326	18.747776
43.710439	1441.889388	18.752794
43.836928	1459.734910	18.757811
44.083426	1459.571076	18.762829
43.971875	1464.338936	18.767847
43.972633	1472.652688	18.772864
44.382221	1474.706661	18.777882
44.209095	1470.999301	18.782899
44.554818	1466.930652	18.787917
44.484627	1477.303081	18.792935
44.465907	1460.735237	18.797952
44.561737	1463.939914	18.802970
44.738400	1469.731255	18.807987
44.437550	1434.467680	18.813005
44.139853	1442.759880	18.818023
44.332527	1458.267045	18.823040
44.802652	1450.910203	18.828058
44.576003	1460.183245	18.833075
45.038788	1464.427519	18.838093
44.870716	1470.446472	18.843111
44.830890	1464.004482	18.848128
44.993799	1452.830460	18.853146
44.543748	1458.588372	18.858163
44.777337	1455.493039	18.863181
44.719874	1464.924910	18.868199
44.852838	1471.684949	18.873216
45.071505	1462.806887	18.878234
44.975459	1474.388925	18.883251
45.138595	1470.686619	18.888269
45.249255	1463.705663	18.893287
45.192046	1472.911939	18.898304
45.001004	1465.082935	18.903322
44.954439	1472.359579	18.908339
45.194295	1466.630121	18.913357
45.032919	1468.725695	18.918375
45.118668	1466.627289	18.923392
45.083913	1478.821948	18.928410
44.859031	1493.711633	18.933427
45.552088	1487.395145	18.938445
45.333275	1491.971713	18.943463
45.787058	1495.501050	18.948480
45.740125	1482.278906	18.953498
45.505759	1489.842461	18.958515
45.737687	1483.684250	18.963533
45.168317	1485.664990	18.968551
45.920649	1488.918447	18.973568
45.719464	1478.908352	18.978586
45.429357	1492.606821	18.983603
45.956539	1512.539821	18.988621
46.213919	1512.961114	18.993639
46.071790	1502.323418	18.998656
46.347313	1518.644199	19.003674
46.395972	1520.263402	19.008691
46.516529	1507.539076	19.013709
46.588983	1503.413424	19.018727
46.297370	1494.186854	19.023744
46.523018	1473.775807	19.028762
45.993001	1474.669094	19.033779
46.465405	1483.805770	19.038797
47.074656	1498.715866	19.043815
46.762994	1494.821186	19.048832
46.570011	1478.923957	19.053850
46.488504	1475.813966	19.058867
46.526642	1468.967021	19.063885
46.515645	1494.135045	19.068903
46.661670	1494.826277	19.073920
47.074662	1501.463491	19.078938
46.821147	1506.613041	19.083955
46.941970	1504.493875	19.088973
46.566645	1506.770261	19.093991
46.482212	1504.424617	19.099008
46.908704	1494.116722	19.104026
46.833449	1507.853903	19.109043
46.758178	1502.472921	19.114061
46.655762	1491.961524	19.119079
46.787594	1521.336295	19.124096
47.344935	1527.643411	19.129114
47.355119	1533.800232	19.134131
47.823563	1522.621135	19.139149
47.705717	1533.413231	19.144167
47.886419	1530.219748	19.149184
47.693914	1529.547043	19.154202
47.431994	1529.882914	19.159219
47.572687	1529.561982	19.164237
47.930808	1532.242098	19.169255
47.648501	1525.980093	19.174272
48.293310	1518.766771	19.179290
47.449337	1520.773997	19.184307
47.733876	1520.407054	19.189325
47.818171	1521.151986	19.194343
47.542749	1529.185469	19.199360
47.877740	1509.643387	19.204378
47.478544	1529.102217	19.209395
47.890758	1530.380479	19.214413
48.137825	1521.388650	19.219431
47.777408	1533.934174	19.224448
47.898943	1533.608534	19.229466
48.092228	1552.504002	19.234483
48.421298	1554.697061	19.239501
48.247773	1560.680538	19.244519
48.229807	1559.877822	19.249536
48.413328	1560.388673	19.254554
48.370893	1560.129887	19.259571
48.464767	1552.104171	19.264589
48.306310	1554.080197	19.269607
48.330539	1547.889953	19.274624
48.511573	1543.554641	19.279642
48.304132	1556.419738	19.284659
49.002061	1570.816304	19.289677
48.963041	1566.820654	19.294695
48.839449	1562.867126	19.299712
48.919633	1543.681434	19.304730
49.157023	1559.083688	19.309747
49.095175	1559.684291	19.314765
49.152883	1545.678962	19.319783
48.796392	1554.826883	19.324800
49.087038	1564.192237	19.329818
49.085177	1580.145197	19.334835
49.083656	1575.003937	19.339853
49.477711	1575.565813	19.344871
49.067647	1586.602271	19.349888
49.086231	1578.436247	19.354906
48.951164	1583.256252	19.359923
49.171807	1579.526900	19.364941
49.828578	1572.063185	19.369959
49.190723	1585.745589	19.374976
49.024672	1587.740588	19.379994
49.583680	1599.509513	19.385011
49.993254	1605.592097	19.390029
50.161445	1610.828470	19.395047
50.120133	1601.689590	19.400064
50.200065	1599.316968	19.405082
50.434432	1576.550725	19.410099
50.482321	1557.641771	19.415117
50.347622	1561.743894	19.420135
50.247597	1559.728725	19.425152
50.372276	1553.206569	19.430170
50.231779	1560.349781	19.435187
50.053929	1554.697780	19.440205
50.086286	1559.960912	19.445223
49.926193	1560.105964	19.450240
49.977561	1553.951976	19.455258
49.847998	1571.168969	19.460275
49.897160	1583.034138	19.465293
50.429491	1578.915925	19.470311
50.242634	1593.130813	19.475328
50.707688	1588.855627	19.480346
50.793792	1586.383575	19.485363
50.629204	1589.827938	19.490381
50.613408	1581.271782	19.495399
50.678182	1598.674970	19.500416
50.834067	1604.691222	19.505434
50.940634	1616.517801	19.510451
51.182768	1616.920951	19.515469
50.943617	1622.152602	19.520487
50.687595	1624.710825	19.525504
51.464888	1617.300588	19.530522
51.085023	1621.336758	19.535539
51.273959	1620.029636	19.540557
50.905190	1610.125680	19.545575
51.045893	1618.089068	19.550592
51.180039	1615.886200	19.555610
51.076712	1618.716000	19.560627
51.126510	1613.665053	19.565645
51.401151	1638.672740	19.570663
51.590624	1641.178607	19.575680
51.910838	1642.282342	19.580698
51.892741	1642.794824	19.585715
51.918156	1651.558279	19.590733
51.753454	1638.583385	19.595751
51.725443	1636.729118	19.600768
51.950121	1635.984320	19.605786
51.881631	1630.375431	19.610803
51.974292	1637.271911	19.615821
52.315020	1632.820039	19.620839
51.923185	1630.582449	19.625856
52.187813	1626.415953	19.630874
52.373135	1633.935814	19.635891
52.529090	1636.179143	19.640909
52.315986	1627.945684	19.645927
52.471616	1633.713205	19.650944
52.318425	1620.366394	19.655962
52.499567	1624.807037	19.660979
52.144198	1626.341265	19.665997
52.020605	1613.294647	19.671015
51.966864	1633.833576	19.676032
52.136113	1627.580562	19.681050
52.360613	1635.880065	19.686067
52.625055	1647.151712	19.691085
52.801707	1654.088250	19.696103
52.658690	1661.378166	19.701120
53.004936	1655.586969	19.706138
53.012353	1659.076340	19.711155
52.621661	1660.529215	19.716173
52.590012	1648.552862	19.721191
52.723210	1661.827049	19.726208
52.882946	1649.887761	19.731226
53.275400	1677.935484	19.736243
53.258268	1684.802300	19.741261
53.654321	1677.087758	19.746279
53.597543	1686.115373	19.751296
54.111845	1673.279985	19.756314
53.689819	1663.977040	19.761331
53.518966	1648.673931	19.766349
53.746717	1643.435911	19.771367
53.504990	1643.473013	19.776384
53.465582	1646.443614	19.781402
53.630009	1645.104324	19.786419
53.771950	1668.104336	19.791437
54.038011	1658.102531	19.796455
54.212833	1669.411049	19.801472
54.182228	1681.854954	19.806490
53.865254	1656.157652	19.811507
53.490593	1663.468330	19.816525
54.211887	1668.339541	19.821543
53.840513	1670.349781	19.826560
53.842217	1674.518752	19.831578
54.132300	1670.873954	19.836595
54.169850	1682.148283	19.841613
54.312188	1669.292485	19.846631
53.871546	1678.625032	19.851648
53.772910	1699.387975	19.856666
54.427708	1691.112823	19.861683
54.401884	1696.950504	19.866701
54.094785	1699.042831	19.871719
54.163486	1709.062783	19.876736
54.619824	1716.255455	19.881754
55.088376	1720.735039	19.886771
54.606991	1731.973518	19.891789
55.319694	1719.879028	19.896807
55.297935	1732.638401	19.901824
55.149542	1717.601162	19.906842
55.170142	1712.125731	19.911859
55.013285	1720.760114	19.916877
55.253998	1721.090085	19.921895
55.346571	1717.753076	19.926912
55.330160	1714.912756	19.931930
55.412488	1713.380164	19.936947
55.174796	1709.052786	19.941965
55.496378	1722.931840	19.946983
55.661960	1718.250455	19.952000
55.464954	1720.874916	19.957018
56.089463	1712.717538	19.962035
55.643839	1715.393120	19.967053
55.748290	1709.693034	19.972071
55.817103	1712.525307	19.977088
55.752026	1710.357315	19.982106
55.921140	1710.854413	19.987123
55.643397	1712.014056	19.992141
55.919296	1715.506509	19.997159
56.031277	1712.594783	20.002176
55.523334	1706.001730	20.007194
56.095587	1711.614028	20.012211
55.923745	1741.994595	20.017229
56.249662	1738.778254	20.022247
56.157899	1740.192367	20.027264
56.284265	1751.381016	20.032282
56.415538	1731.203897	20.037299
56.229311	1734.245030	20.042317
56.240460	1736.707554	20.047335
56.286718	1735.108882	20.052352
56.365684	1731.491674	20.057370
56.344789	1751.397853	20.062387
56.513932	1761.103641	20.067405
56.960070	1757.117917	20.072423
56.833515	1756.689980	20.077440
56.930333	1768.617685	20.082458
56.994836	1759.156736	20.087475
56.781849	1765.572350	20.092493
57.199372	1771.443280	20.097511
57.083528	1760.848300	20.102528
56.993003	1757.195125	20.107546
57.221949	1758.130312	20.112563
57.276954	1770.716816	20.117581
57.537776	1772.809585	20.122599
57.774495	1778.238997	20.127616
57.413514	1779.645639	20.132634
57.396560	1765.503057	20.137651
57.597766	1787.251875	20.142669
57.972207	1787.571362	20.147687
58.145298	1778.057619	20.152704
57.738590	1783.019215	20.157722
58.409531	1772.003895	20.162739
58.015818	1763.816741	20.167757
57.782717	1758.271813	20.172775
57.982129	1749.396965	20.177792
57.379841	1773.434765	20.182810
57.935036	1777.303271	20.187827
57.740947	1779.172038	20.192845
58.013340	1774.742048	20.197863
58.029521	1781.863802	20.202880
58.061131	1803.895362	20.207898
58.148024	1797.839723	20.212915
58.512412	1807.490445	20.217933
58.457820	1819.904374	20.222951
58.391689	1814.067497	20.227968
58.469993	1807.466686	20.232986
58.627800	1806.752811	20.238003
58.887325	1800.922551	20.243021
59.040567	1799.150110	20.248039
59.134262	1806.240565	20.253056
58.849352	1807.722817	20.258074
58.957536	1791.744201	20.263091
58.766341	1802.945999	20.268109
58.745291	1807.452977	20.273127
58.959170	1820.053419	20.278144
59.176371	1833.203848	20.283162
59.594989	1814.611225	20.288179
59.498445	1825.022689	20.293197
59.522513	1824.023666	20.298215
59.472416	1803.623894	20.303232
59.441725	1822.578159	20.308250
59.358942	1816.446431	20.313267
59.469620	1812.482469	20.318285
59.584041	1814.651792	20.323303
59.938961	1820.944455	20.328320
59.859349	1828.672343	20.333338
60.103141	1809.193963	20.338355
59.913909	1823.322654	20.343373
59.695142	1827.802672	20.348391
60.026767	1806.854443	20.353408
60.024292	1822.302503	20.358426
59.916359	1811.202500	20.363443
60.023599	1824.413213	20.368461
59.799442	1845.036090	20.373479
60.152348	1853.742788	20.378496
60.106174	1849.891537	20.383514
60.093404	1849.191675	20.388531
60.125011	1853.360477	20.393549
60.206711	1860.120695	20.398567
61.203615	1857.601230	20.403584
60.566165	1866.137966	20.408602
61.038892	1857.618435	20.413619
61.097006	1864.219580	20.418637
61.547646	1865.077791	20.423655
61.316709	1841.569638	20.428672
60.944020	1838.688968	20.433690
61.307270	1830.928793	20.438707
61.120968	1829.289220	20.443725
61.115605	1830.447754	20.448743
61.266321	1828.517085	20.453760
60.951643	1838.883905	20.458778
61.566285	1847.301709	20.463795
61.279152	1858.686899	20.468813
61.145277	1870.779561	20.473831
61.340616	1851.171552	20.478848
61.040847	1857.774162	20.483866
61.451177	1859.404101	20.488883
61.419330	1868.303505	20.493901
61.277436	1868.616792	20.498919
61.631139	1879.949246	20.503936
61.860344	1884.329273	20.508954
62.062721	1887.721133	20.513971
61.838314	1898.030561	20.518989
61.752745	1899.148817	20.524007
61.917390	1883.134204	20.529024
61.915973	1900.808484	20.534042
62.438477	1903.818352	20.539059
62.179952	1918.598862	20.544077
62.051999	1924.111222	20.549095
62.471233	1921.188050	20.554112
62.390854	1927.045265	20.559130
62.636815	1913.538551	20.564147
62.403253	1916.659187	20.569165
62.688379	1918.311987	20.574183
62.559544	1913.672502	20.579200
62.766715	1920.490744	20.584218
63.117036	1920.839612	20.589235
62.988135	1919.171845	20.594253
63.146219	1926.341863	20.599271
63.066668	1928.870580	20.604288
63.218060	1944.105759	20.609306
63.370258	1940.570288	20.614323
63.669417	1942.978954	20.619341
63.642658	1930.609294	20.624359
63.421223	1910.568364	20.629376
63.174678	1916.926405	20.634394
63.458469	1918.052714	20.639411
63.809554	1931.444065	20.644429
63.818188	1933.410242	20.649447
63.950302	1928.239893	20.654464
63.479484	1926.461321	20.659482
63.587578	1924.660307	20.664499
63.641259	1928.568424	20.669517
63.168269	1932.635808	20.674535
63.412744	1926.805036	20.679552
63.410806	1938.248657	20.684570
63.928555	1960.595340	20.689587
63.966530	1958.307146	20.694605
64.283447	1959.815933	20.699623
64.321771	1965.296107	20.704640
64.496703	1953.321596	20.709658
64.401075	1956.119677	20.714675
64.527005	1954.416095	20.719693
64.621299	1953.583983	20.724711
64.739188	1943.326392	20.729728
64.514087	1958.669857	20.734746
64.755505	1943.913416	20.739763
64.468011	1955.997281	20.744781
64.734969	1981.673259	20.749799
65.197311	1974.705407	20.754816
65.224755	1989.173010	20.759834
65.149558	1982.869114	20.764851
65.698605	1980.618105	20.769869
65.679691	1984.438637	20.774887
65.612416	1966.610890	20.779904
65.228031	1971.704669	20.784922
65.628552	1977.843420	20.789939
65.787063	1955.652083	20.794957
65.280844	1959.483456	20.799975
65.751184	1972.148523	20.804992
65.696959	1984.323574	20.810010
65.559760	1982.143054	20.815027
65.817893	1979.713370	20.820045
65.753384	1981.785724	20.825063
66.043572	1973.064824	20.830080
65.897456	1985.830981	20.835098
65.691634	1975.312722	20.840115
65.876942	1980.961505	20.845133
65.780184	1983.873938	20.850151
66.086237	1993.713138	20.855168
66.402996	2011.420785	20.860186
66.633939	2011.104023	20.865203
66.239367	2011.367541	20.870221
65.947508	2014.904872	20.875239
66.776744	2005.795304	20.880256
66.413227	2010.057784	20.885274
66.410419	2004.631978	20.890291
66.352799	2015.249910	20.895309
66.521804	2032.200584	20.900327
66.987294	2034.829784	20.905344
66.822211	2032.938874	20.910362
67.397422	2019.130247	20.915379
67.475239	2030.503087	20.920397
66.896931	2029.962214	20.925415
67.089146	2019.563957	20.930432
67.311060	2027.824341	20.935450
67.175416	2028.550727	20.940467
67.653168	2018.507410	20.945485
67.608760	2023.782992	20.950503
67.456645	2018.993599	20.955520
67.677759	2021.766121	20.960538
67.808101	2027.580483	20.965555
68.261126	2035.860156	20.970573
68.090149	2042.259691	20.975591
68.051719	2023.960232	20.980608
67.704305	2022.964320	20.985626
67.965315	2029.741041	20.990643
68.272128	2033.488865	20.995661
68.045234	2039.417179	21.000679
68.335280	2038.097252	21.005696
68.122661	2029.894989	21.010714
68.195593	2040.693312	21.015731
68.379825	2039.999663	21.020749
68.167836	2040.733942	21.025767
68.177393	2029.655701	21.030784
68.142276	2034.256005	21.035802
68.201472	2062.515784	21.040819
68.425466	2053.905372	21.045837
68.380155	2057.359063	21.050855
69.120605	2063.456243	21.055872
68.867554	2064.663795	21.060890
69.142218	2054.743177	21.065907
69.418517	2065.002454	21.070925
69.625584	2065.927302	21.075943
69.319928	2054.624781	21.080960
69.505834	2051.556303	21.085978
69.415910	2052.566443	21.090995
69.732035	2045.559342	21.096013
69.538194	2055.010370	21.101031
69.282047	2050.217096	21.106048
69.810628	2057.137784	21.111066
69.253768	2087.584622	21.116083
69.771158	2080.669234	21.121101
69.335885	2077.976991	21.126119
69.845378	2069.944919	21.131136
69.936589	2076.660358	21.136154
69.635950	2083.759416	21.141171
70.221735	2087.288337	21.146189
70.332897	2099.672346	21.151207
70.398985	2103.770170	21.156224
70.444162	2108.920163	21.161242
70.698545	2103.728369	21.166259
70.796514	2099.566061	21.171277
70.691805	2108.778794	21.176295
70.815196	2108.695922	21.181312
71.055437	2096.692990	21.186330
70.596133	2091.798643	21.191347
70.873002	2105.663780	21.196365
70.882261	2095.994453	21.201383
70.899884	2094.391618	21.206400
71.150456	2101.516320	21.211418
70.997548	2096.488672	21.216435
71.172626	2099.299324	21.221453
70.956531	2104.973739	21.226471
71.124249	2097.716165	21.231488
71.455712	2112.943998	21.236506
71.008933	2127.519028	21.241523
71.751633	2115.386405	21.246541
71.534649	2134.850333	21.251559
71.811565	2128.385643	21.256576
71.829427	2129.613190	21.261594
71.968308	2130.152696	21.266611
71.906692	2122.412981	21.271629
71.826026	2123.115130	21.276647
72.246527	2125.328596	21.281664
72.257481	2123.620965	21.286682
71.978453	2122.220479	21.291699
71.867180	2128.454098	21.296717
72.108295	2136.188191	21.301735
72.317367	2155.141235	21.306752
72.323534	2157.973707	21.311770
72.308680	2159.311573	21.316787
72.723021	2159.533738	21.321805
72.438965	2164.952306	21.326823
72.189884	2162.369423	21.331840
72.642435	2164.365415	21.336858
72.854658	2180.937494	21.341875
72.864336	2182.279772	21.346893
73.018488	2179.786343	21.351911
73.100488	2176.528730	21.356928
73.422472	2170.386072	21.361946
73.736916	2172.477713	21.366963
73.790192	2166.954008	21.371981
73.909021	2170.914998	21.376999
73.490257	2169.038040	21.382016
73.729683	2161.148373	21.387034
73.578779	2169.353915	21.392051
73.588657	2162.734932	21.397069
73.786789	2161.410894	21.402087
73.793216	2154.118338	21.407104
74.157988	2157.813313	21.412122
74.084121	2164.008288	21.417139
73.991376	2158.440218	21.422157
74.153654	2164.695178	21.427175
74.165228	2154.867769	21.432192
74.571690	2148.527516	21.437210
73.842761	2169.394457	21.442227
74.043009	2154.654263	21.447245
74.022203	2165.650035	21.452263
74.065836	2185.903361	21.457280
74.281419	2194.516028	21.462298
74.112093	2198.085903	21.467315
74.601441	2207.037357	21.472333
75.135427	2214.407574	21.477351
75.241142	2212.713406	21.482368
75.561293	2209.353645	21.487386
74.990503	2221.311908	21.492403
75.640789	2214.890791	21.497421
75.499050	2206.495046	21.502439
75.682700	2205.419043	21.507456
75.560279	2195.991863	21.512474
75.447307	2182.460375	21.517491
75.582365	2191.031431	21.522509
75.548495	2202.355734	21.527527
75.675795	2202.258438	21.532544
75.671874	2212.718040	21.537562
75.713966	2209.302464	21.542579
75.823111	2205.124306	21.547597
75.714002	2209.511123	21.552615
75.661618	2208.841411	21.557632
75.873357	2206.527616	21.562650
75.798454	2233.914678	21.567667
76.059313	2230.090542	21.572685
76.070220	2238.027475	21.577703
76.359055	2241.913742	21.582720
76.200879	2232.415290	21.587738
76.273701	2256.149188	21.592755
76.502917	2257.033384	21.597773
76.926679	2254.003507	21.602791
76.941325	2260.423439	21.607808
77.340649	2256.131575	21.612826
76.932090	2261.914418	21.617843
77.255534	2246.391251	21.622861
76.904806	2250.228691	21.627879
76.658584	2251.123148	21.632896
77.190560	2253.252864	21.637914
77.332821	2283.619205	21.642931
77.149861	2286.940983	21.647949
77.315172	2279.192429	21.652967
77.255917	2296.748778	21.657984
77.944925	2286.715061	21.663002
77.431591	2287.709756	21.668019
77.579407	2291.152057	21.673037
77.740620	2296.793523	21.678055
77.673326	2289.196381	21.683072
78.221497	2300.936344	21.688090
78.176181	2306.946753	21.693107
77.951424	2308.182518	21.698125
78.308149	2311.478699	21.703143
78.117017	2306.759830	21.708160
78.474992	2301.462672	21.713178
78.352441	2308.822732	21.718195
78.187771	2294.801899	21.723213
78.494166	2304.634747	21.728231
78.633162	2331.334332	21.733248
78.925474	2320.067833	21.738266
79.007351	2333.753606	21.743283
78.952413	2334.079499	21.748301
79.502126	2323.226723	21.753319
79.521456	2337.548173	21.758336
79.402055	2330.402300	21.763354
79.451575	2326.262503	21.768371
79.232297	2324.778114	21.773389
79.442896	2329.145794	21.778407
79.546072	2336.886248	21.783424
79.862314	2312.817511	21.788442
79.741621	2316.564006	21.793459
79.645458	2324.466713	21.798477
79.713843	2324.930284	21.803495
79.735499	2326.632769	21.808512
79.566503	2322.195645	21.813530
79.934835	2329.291349	21.818547
79.906690	2338.640177	21.823565
80.236687	2354.679248	21.828583
80.226315	2361.671811	21.833600
80.281192	2348.298647	21.838618
80.210081	2362.917915	21.843635
80.193031	2359.445942	21.848653
80.460822	2360.445610	21.853671
80.530096	2386.686183	21.858688
80.778097	2380.497011	21.863706
80.941328	2391.540479	21.868723
80.917860	2386.305142	21.873741
81.291193	2381.200875	21.878759
80.778848	2379.566303	21.883776
80.669819	2372.977901	21.888794
81.115190	2390.353736	21.893811
81.082043	2399.623906	21.898829
81.365729	2401.750383	21.903847
81.237211	2393.738343	21.908864
81.506924	2391.190550	21.913882
81.420455	2402.591797	21.918899
81.405015	2408.327843	21.923917
81.766850	2431.656015	21.928935
81.948769	2432.574413	21.933952
81.989022	2423.012742	21.938970
82.140401	2429.678042	21.943987
81.882473	2428.991895	21.949005
82.370769	2418.829068	21.954023
82.259175	2431.282826	21.959040
82.592818	2419.947226	21.964058
82.813103	2437.406957	21.969075
82.518881	2434.429354	21.974093
83.180859	2429.482477	21.979111
83.136614	2431.156102	21.984128
82.946950	2416.384821	21.989146
82.776507	2422.751160	21.994163
82.781655	2436.382582	21.999181
83.149704	2432.271414	22.004199
82.632426	2451.502904	22.009216
83.199327	2458.025151	22.014234
83.423327	2436.989335	22.019251
83.252236	2443.699069	22.024269
83.610571	2433.245528	22.029287
83.342814	2448.244980	22.034304
83.562413	2435.474786	22.039322
83.436216	2435.270571	22.044339
83.495679	2457.551986	22.049357
83.791035	2463.702406	22.054375
84.230842	2477.715155	22.059392
84.130288	2460.674558	22.064410
83.988484	2474.225777	22.069427
83.919720	2474.596474	22.074445
84.035152	2462.654824	22.079463
84.037505	2475.415551	22.084480
84.097775	2479.241820	22.089498
84.403382	2482.626793	22.094515
84.537475	2500.808264	22.099533
84.724363	2492.448211	22.104551
84.694542	2491.890693	22.109568
85.093549	2495.288384	22.114586
84.902085	2484.198155	22.119603
84.579725	2495.130024	22.124621
85.016003	2510.343293	22.129639
85.220419	2521.856785	22.134656
85.120972	2528.667701	22.139674
85.536337	2514.619516	22.144691
85.142358	2517.109742	22.149709
85.092554	2519.387202	22.154727
85.266365	2526.692490	22.159744
85.740348	2544.453308	22.164762
86.001821	2537.647326	22.169779
86.233056	2541.076686	22.174797
86.202266	2545.178432	22.179815
86.151774	2544.827463	22.184832
86.245759	2536.186303	22.189850
86.368568	2547.053898	22.194867
86.421154	2545.612157	22.199885
86.322782	2534.997615	22.204903
86.638469	2536.997770	22.209920
86.421734	2540.580675	22.214938
86.306018	2548.265877	22.219955
86.325121	2561.336680	22.224973
86.785166	2561.768609	22.229991
86.766271	2578.003940	22.235008
86.801055	2570.346882	22.240026
87.005822	2569.684265	22.245043
86.916741	2574.349548	22.250061
86.981785	2582.433214	22.255079
87.476473	2594.518829	22.260096
87.197597	2601.146843	22.265114
87.602341	2597.295298	22.270131
87.413377	2598.529501	22.275149
87.587849	2592.551200	22.280167
87.841629	2605.703332	22.285184
87.530010	2617.743670	22.290202
88.090590	2612.167670	22.295219
88.128320	2624.140641	22.300237
88.613185	2612.342147	22.305255
88.137872	2623.174389	22.310272
88.256110	2614.483510	22.315290
88.557348	2606.469829	22.320307
88.587947	2614.569045	22.325325
88.925014	2611.466424	22.330343
88.577242	2609.351711	22.335360
88.451973	2615.235894	22.340378
88.827563	2603.067301	22.345395
88.724291	2613.755388	22.350413
88.908564	2632.340111	22.355431
88.886191	2640.123116	22.360448
89.213005	2638.036486	22.365466
89.434257	2643.673472	22.370483
89.470346	2647.443744	22.375501
89.373610	2635.782475	22.380519
89.147764	2639.442297	22.385536
89.389437	2640.307530	22.390554
89.622158	2629.205762	22.395571
89.366030	2656.249921	22.400589
89.837023	2664.359064	22.405607
89.930821	2661.906040	22.410624
89.973887	2678.399331	22.415642
90.328934	2665.290248	22.420659
89.653930	2668.335956	22.425677
90.116333	2667.441601	22.430695
90.433287	2674.393209	22.435712
90.422389	2687.925149	22.440730
90.868253	2686.723310	22.445747
90.858134	2677.853619	22.450765
90.853936	2677.405633	22.455783
91.432278	2684.664032	22.460800
90.939302	2686.026621	22.465818
91.212471	2677.945499	22.470835
90.903646	2683.190791	22.475853
91.340171	2676.036748	22.480871
91.134658	2681.913548	22.485888
91.048045	2679.804486	22.490906
91.332386	2688.464923	22.495923
91.611437	2709.130596	22.500941
91.611670	2706.434774	22.505959
92.105216	2700.646999	22.510976
91.819401	2704.054360	22.515994
92.145901	2704.046973	22.521011
92.053556	2703.760787	22.526029
92.132583	2694.171676	22.531047
92.334080	2684.750511	22.536064
92.112253	2696.197567	22.541082
92.422277	2701.209512	22.546099
92.310119	2717.540120	22.551117
92.568352	2722.519688	22.556135
92.693825	2725.370146	22.561152
92.630600	2710.323376	22.566170
93.058733	2708.231214	22.571187
92.763172	2726.721925	22.576205
92.699660	2735.564270	22.581223
93.145710	2748.610742	22.586240
93.003302	2763.862998	22.591258
92.937021	2754.082520	22.596275
93.458821	2756.549797	22.601293
93.517029	2755.369887	22.606311
93.754555	2760.931200	22.611328
93.575835	2780.778177	22.616346
93.812585	2774.909980	22.621363
93.961091	2774.457229	22.626381
94.301776	2764.611859	22.631399
94.227014	2776.617710	22.636416
94.197957	2778.569751	22.641434
94.549424	2760.208142	22.646451
94.461451	2779.783051	22.651469
94.392090	2774.828771	22.656487
94.455313	2773.229551	22.661504
94.361182	2772.936572	22.666522
94.535050	2783.999036	22.671539
94.682885	2797.329459	22.676557
94.613129	2801.429444	22.681575
95.011109	2806.417835	22.686592
95.009539	2800.072503	22.691610
95.018977	2800.662752	22.696627
95.142449	2809.739974	22.701645
95.322921	2821.171037	22.706663
95.372789	2827.042502	22.711680
95.628903	2825.824766	22.716698
95.965125	2825.140219	22.721715
95.817971	2826.198840	22.726733
95.864529	2819.373919	22.731751
95.896728	2822.338228	22.736768
96.056567	2815.726074	22.741786
95.715394	2816.835256	22.746803
95.974079	2837.893029	22.751821
96.426925	2850.707375	22.756839
96.369499	2850.485096	22.761856
96.480336	2860.517141	22.766874
96.618115	2849.993078	22.771891
96.723899	2843.426850	22.776909
96.536481	2854.907706	22.781927
96.703315	2848.389258	22.786944
96.763291	2868.146514	22.791962
97.186830	2875.585299	22.796979
97.349882	2870.170954	22.801997
97.489904	2876.991269	22.807015
97.514470	2882.744895	22.812032
97.449113	2886.721347	22.817050
97.414257	2866.823531	22.822067
97.554416	2876.947586	22.827085
97.429391	2889.153158	22.832103
97.989849	2893.226193	22.837120
97.756973	2911.988247	22.842138
98.166921	2896.778860	22.847155
97.961663	2908.162314	22.852173
98.034564	2908.656652	22.857191
98.270441	2909.705527	22.862208
98.404335	2926.929509	22.867226
98.901840	2928.575674	22.872243
98.856314	2927.555798	22.877261
98.641006	2923.368070	22.882279
99.274631	2911.212108	22.887296
98.979415	2909.378023	22.892314
99.051680	2920.090856	22.897331
99.046870	2919.930745	22.902349
99.284595	2924.086643	22.907367
99.384558	2921.394776	22.912384
99.708830	2935.317393	22.917402
99.749759	2931.119211	22.922419
99.777712	2952.166448	22.927437
99.683885	2952.364731	22.932455
99.980553	2945.241746	22.937472
99.881841	2958.265819	22.942490
100.150221	2952.995450	22.947507
100.025683	2953.930269	22.952525
99.725231	2954.601256	22.957543
99.919716	2958.211184	22.962560
100.310663	2973.077892	22.967578
100.182539	2982.475910	22.972595
100.153298	2972.898218	22.977613
100.358163	2996.365383	22.982631
100.732658	3005.841774	22.987648
100.837848	3007.040591	22.992666
101.090495	3008.056781	22.997683
100.925412	3013.455589	23.002701
100.749746	3014.623260	23.007719
101.185795	3032.323787	23.012736
101.135877	3044.181257	23.017754
101.485005	3028.585351	23.022771
101.440262	3029.410931	23.027789
101.458408	3034.041705	23.032807
102.091398	3042.649455	23.037824
101.936755	3050.418894	23.042842
102.391333	3053.772884	23.047859
102.967100	3047.919822	23.052877
102.990965	3033.194160	23.057895
103.200855	3013.469877	23.062912
102.938402	3017.514756	23.067930
102.614075	3018.130245	23.072947
102.718967	3012.762860	23.077965
102.658068	3010.458960	23.082983
102.882515	3013.197452	23.088000
102.902540	3007.801575	23.093018
102.815425	3017.454638	23.098035
103.004480	3032.329567	23.103053
102.870514	3039.565685	23.108071
103.139425	3041.795675	23.113088
103.027701	3044.214541	23.118106
103.088378	3052.861356	23.123123
103.286517	3067.057286	23.128141
103.210367	3073.340990	23.133159
103.572142	3074.972592	23.138176
103.721497	3110.904918	23.143194
103.903841	3103.237781	23.148211
104.026064	3106.396709	23.153229
103.617029	3111.688230	23.158247
104.407589	3117.254349	23.163264
104.232211	3141.436903	23.168282
104.455201	3137.450306	23.173299
104.858193	3128.178642	23.178317
104.947803	3136.072718	23.183335
104.666823	3124.302357	23.188352
104.981262	3143.565177	23.193370
105.053712	3162.619590	23.198387
105.782670	3158.607254	23.203405
105.373581	3155.514833	23.208423
105.602612	3159.291929	23.213440
105.391321	3161.451683	23.218458
105.640320	3156.038390	23.223475
106.266153	3153.811933	23.228493
106.056057	3150.490181	23.233511
105.987994	3154.092359	23.238528
105.961096	3142.398894	23.243546
106.056663	3155.949673	23.248563
106.437803	3160.324055	23.253581
106.462184	3168.754105	23.258599
106.642272	3174.243172	23.263616
106.886945	3173.311150	23.268634
106.530551	3164.896416	23.273651
106.694580	3176.845010	23.278669
106.441825	3175.443231	23.283687
106.687788	3186.919253	23.288704
107.032299	3203.070980	23.293722
106.939922	3200.746269	23.298739
107.066727	3194.255551	23.303757
107.153237	3209.242474	23.308775
107.555410	3213.507887	23.313792
107.838033	3216.196253	23.318810
107.794961	3220.391149	23.323827
108.141406	3216.540033	23.328845
107.862943	3219.778579	23.333863
108.324879	3211.529773	23.338880
108.129322	3222.078020	23.343898
108.286382	3217.619634	23.348915
108.561377	3233.783273	23.353933
108.708649	3246.390575	23.358951
108.957290	3245.037433	23.363968
108.892210	3253.694117	23.368986
108.883390	3260.725017	23.374003
109.182100	3239.842101	23.379021
109.174701	3246.316478	23.384039
109.296452	3238.708498	23.389056
109.344043	3243.089201	23.394074
109.094518	3252.746019	23.399091
109.417438	3237.627843	23.404109
109.268929	3241.359473	23.409127
109.643898	3255.733044	23.414144
109.893219	3263.246080	23.419162
109.312157	3267.295640	23.424179
109.726693	3267.517009	23.429197
109.270730	3283.729831	23.434215
109.604423	3287.396359	23.439232
109.778066	3293.081017	23.444250
110.037810	3313.844782	23.449267
110.305044	3319.749019	23.454285
110.488934	3325.867025	23.459303
110.460198	3331.319396	23.464320
110.865180	3321.128019	23.469338
111.067853	3349.214477	23.474355
111.479937	3349.008309	23.479373
111.417710	3348.873035	23.484391
111.278749	3344.518250	23.489408
111.611811	3350.424219	23.494426
111.562624	3341.222028	23.499443
111.535607	3344.707628	23.504461
111.746357	3346.195322	23.509479
111.627773	3340.169097	23.514496
111.993443	3361.299272	23.519514
111.885672	3366.656056	23.524531
112.195368	3370.624989	23.529549
112.139263	3380.202683	23.534567
112.164795	3367.740950	23.539584
112.226948	3387.881178	23.544602
112.032860	3411.197575	23.549619
112.403604	3399.588208	23.554637
112.729781	3412.737727	23.559655
113.026639	3435.999810	23.564672
113.046273	3432.954205	23.569690
112.941882	3428.401561	23.574707
113.357364	3422.895313	23.579725
113.636293	3426.408723	23.584743
114.085680	3450.122387	23.589760
114.253546	3443.822021	23.594778
114.261266	3431.696640	23.599795
114.298861	3418.352178	23.604813
114.281097	3424.094496	23.609831
114.305411	3432.628636	23.614848
114.218149	3443.134337	23.619866
114.457323	3454.540421	23.624883
114.652979	3451.935011	23.629901
114.577875	3449.444420	23.634919
114.809212	3442.247360	23.639936
115.034535	3452.619527	23.644954
114.835647	3442.192425	23.649971
114.986890	3437.620766	23.654989
115.112821	3472.197979	23.660007
114.987506	3477.164398	23.665024
115.185985	3469.803071	23.670042
115.188695	3480.589202	23.675059
115.377028	3483.015246	23.680077
115.553182	3499.426201	23.685095
115.545595	3503.153505	23.690112
115.560948	3493.189387	23.695130
116.087787	3507.597153	23.700147
116.196531	3521.300403	23.705165
116.405438	3525.428942	23.710183
116.587543	3529.633565	23.715200
116.696030	3524.576036	23.720218
116.760308	3530.009170	23.725235
116.839292	3515.075126	23.730253
116.790945	3523.907934	23.735271
116.753638	3516.969794	23.740288
117.153410	3522.992758	23.745306
117.543808	3550.720614	23.750323
117.571773	3558.351865	23.755341
117.538416	3548.940638	23.760359
117.500981	3558.633072	23.765376
118.085774	3552.906678	23.770394
117.685672	3550.674888	23.775411
117.980506	3551.964458	23.780429
118.252478	3557.092420	23.785447
118.093821	3554.484909	23.790464
118.033174	3550.674601	23.795482
118.156261	3570.254608	23.800499
118.215749	3568.264195	23.805517
118.358878	3566.255630	23.810535
118.337194	3588.150903	23.815552
118.691763	3592.929404	23.820570
118.776443	3597.772580	23.825587
118.820383	3606.255148	23.830605
119.208881	3611.173716	23.835623
119.608738	3614.363645	23.840640
119.739888	3629.869186	23.845658
119.636867	3631.374109	23.850675
119.943313	3622.573616	23.855693
119.970382	3631.722762	23.860711
119.651199	3631.835849	23.865728
119.878693	3622.492105	23.870746
120.036684	3632.757803	23.875763
120.420384	3650.536587	23.880781
120.568064	3657.274092	23.885799
120.341301	3662.421506	23.890816
120.602177	3656.599779	23.895834
120.301482	3655.829104	23.900851
120.769357	3663.048742	23.905869
120.935004	3689.165166	23.910887
120.778705	3685.214724	23.915904
121.324460	3685.191979	23.920922
121.081226	3702.206304	23.925939
121.353552	3709.360245	23.930957
121.462604	3708.716744	23.935975
121.393916	3727.780999	23.940992
121.840624	3723.828547	23.946010
121.757631	3733.923894	23.951027
121.773585	3746.189521	23.956045
122.148220	3746.111193	23.961063
122.303269	3744.719536	23.966080
122.378387	3756.551378	23.971098
122.603607	3763.904073	23.976115
123.022402	3760.596384	23.981133
123.141447	3767.794970	23.986151
123.068823	3764.573993	23.991168
123.454720	3759.724488	23.996186
123.731043	3768.329377	24.001203
123.500359	3754.354938	24.006221
123.685902	3756.394084	24.011239
123.584248	3766.515765	24.016256
123.793088	3758.791171	24.021274
123.633675	3773.598407	24.026291
123.805824	3787.314644	24.031309
124.022149	3783.890011	24.036327
123.850667	3785.704295	24.041344
124.143989	3797.439088	24.046362
124.266070	3814.562466	24.051379
123.973550	3817.832592	24.056397
124.418139	3811.994231	24.061415
124.327559	3824.008229	24.066432
124.704719	3842.616275	24.071450
124.952743	3845.265194	24.076467
125.018221	3846.172210	24.081485
125.259561	3850.172642	24.086503
125.156099	3850.584340	24.091520
125.455685	3867.992623	24.096538
125.818978	3874.738297	24.101555
125.713022	3882.598138	24.106573
126.050688	3861.144560	24.111591
126.139324	3871.969914	24.116608
126.281043	3866.681584	24.121626
126.438037	3850.059900	24.126643
126.165115	3857.304396	24.131661
126.958632	3877.862608	24.136679
126.660368	3885.201464	24.141696
126.948240	3888.443814	24.146714
127.073630	3897.364269	24.151731
126.753540	3888.936841	24.156749
127.413556	3878.926192	24.161767
127.279327	3893.554969	24.166784
127.245885	3906.292670	24.171802
127.334021	3918.831944	24.176819
127.440419	3916.950272	24.181837
128.070055	3911.957295	24.186855
127.760080	3914.054717	24.191872
128.149937	3928.598111	24.196890
128.071719	3939.274702	24.201907
128.177826	3941.184870	24.206925
128.787869	3931.570246	24.211943
128.707715	3942.466454	24.216960
128.331060	3937.068475	24.221978
128.636956	3960.726316	24.226995
128.780135	3967.113512	24.232013
128.960131	3969.107933	24.237031
128.776749	3976.975103	24.242048
129.476079	3981.940858	24.247066
129.404939	3998.649900	24.252083
129.413212	3995.583621	24.257101
129.822527	3990.703404	24.262119
129.575994	4002.006287	24.267136
129.609535	4020.502817	24.272154
130.002845	4017.691029	24.277171
130.177883	4020.496923	24.282189
130.552724	4023.326497	24.287207
130.305183	4039.506058	24.292224
130.829823	4042.794359	24.297242
130.785046	4046.530300	24.302259
130.373534	4044.145200	24.307277
131.152082	4048.472282	24.312295
131.275765	4065.409841	24.317312
131.637954	4067.942294	24.322330
131.479896	4066.483051	24.327347
131.487481	4067.011448	24.332365
131.675260	4071.900731	24.337383
131.668741	4074.328357	24.342400
131.925257	4088.066353	24.347418
132.116963	4096.422801	24.352435
132.079169	4099.315059	24.357453
132.327171	4087.810898	24.362471
132.462465	4090.828102	24.367488
132.504434	4117.463726	24.372506
132.781963	4114.049776	24.377523
132.896410	4122.480817	24.382541
132.991238	4126.961054	24.387559
132.906874	4123.166728	24.392576
133.410894	4117.491275	24.397594
133.480429	4150.240288	24.402611
133.664051	4156.005507	24.407629
133.941169	4140.768037	24.412647
134.073016	4148.531631	24.417664
134.295398	4149.674952	24.422682
134.272031	4142.197599	24.427699
134.158993	4149.928427	24.432717
134.372453	4143.043850	24.437735
134.223300	4148.517192	24.442752
134.598182	4137.732208	24.447770
134.554478	4160.750068	24.452787
134.566469	4170.243766	24.457805
134.922274	4172.723747	24.462823
135.083442	4168.621508	24.467840
134.783845	4153.698223	24.472858
134.885105	4185.303845	24.477875
135.236343	4204.599309	24.482893
135.488825	4202.114312	24.487911
135.447528	4217.335931	24.492928
135.353601	4226.432583	24.497946
135.794569	4235.862132	24.502963
136.061875	4262.148948	24.507981
136.296455	4259.499178	24.512999
136.376773	4272.880217	24.518016
136.647975	4253.046198	24.523034
137.015832	4261.372448	24.528051
137.075943	4275.206451	24.533069
137.487398	4275.891753	24.538087
137.140098	4298.445788	24.543104
137.332052	4287.442493	24.548122
137.753943	4292.745935	24.553139
137.381294	4294.493118	24.558157
137.986066	4288.126127	24.563175
137.842159	4292.349391	24.568192
138.025753	4298.163095	24.573210
138.339366	4311.115052	24.578227
137.984812	4315.928269	24.583245
138.609704	4313.873079	24.588263
138.197563	4308.898959	24.593280
138.435902	4328.648288	24.598298
138.857480	4328.045253	24.603315
138.835158	4340.531461	24.608333
139.195441	4334.963542	24.613351
139.318266	4324.162596	24.618368
139.819962	4352.042005	24.623386
139.907615	4362.613129	24.628403
139.759757	4358.454811	24.633421
139.889106	4358.997352	24.638439
140.044582	4356.823648	24.643456
139.882411	4352.485012	24.648474
140.111569	4358.377041	24.653491
140.387831	4385.790195	24.658509
140.516127	4378.353026	24.663527
140.399529	4384.926632	24.668544
140.584459	4391.434276	24.673562
140.894139	4380.664624	24.678579
140.525958	4401.330441	24.683597
140.986642	4399.740581	24.688615
141.276821	4412.293327	24.693632
141.621143	4431.555175	24.698650
141.933610	4419.598364	24.703667
141.805198	4438.006791	24.708685
141.863169	4440.879745	24.713703
142.320379	4433.706722	24.718720
142.652411	4426.741796	24.723738
142.428405	4440.594938	24.728755
142.221135	4439.305610	24.733773
142.821041	4447.200292	24.738791
142.530970	4455.171556	24.743808
142.570840	4462.486701	24.748826
142.691296	4461.184954	24.753843
142.635130	4469.883757	24.758861
142.887423	4480.311214	24.763879
143.131515	4496.141496	24.768896
143.350042	4498.834380	24.773914
143.491621	4512.774038	24.778931
143.376309	4529.527170	24.783949
143.610342	4518.621489	24.788967
143.865748	4535.667329	24.793984
144.522249	4554.544658	24.799002
144.765041	4548.248004	24.804019
145.036974	4541.052787	24.809037
144.997296	4546.475500	24.814055
145.015750	4545.381555	24.819072
144.655353	4546.257795	24.824090
144.840127	4557.159085	24.829107
145.319401	4574.346334	24.834125
145.473433	4579.475225	24.839143
145.533020	4576.232233	24.844160
145.498422	4578.266522	24.849178
146.204750	4589.813983	24.854195
145.660849	4606.161215	24.859213
145.552648	4598.570881	24.864231
146.002557	4610.615477	24.869248
146.155103	4629.169449	24.874266
146.672239	4628.100588	24.879283
146.501370	4635.015963	24.884301
146.977968	4653.073873	24.889319
147.130366	4654.615829	24.894336
147.122950	4653.452525	24.899354
147.327145	4655.522569	24.904371
146.900084	4668.174347	24.909389
147.195641	4678.502264	24.914407
147.594682	4683.349352	24.919424
147.502361	4694.792225	24.924442
147.870990	4706.933402	24.929459
148.019633	4721.667012	24.934477
148.683575	4717.164607	24.939495
148.928586	4714.059070	24.944512
148.945975	4732.136251	24.949530
149.420923	4736.264073	24.954547
149.507676	4744.056283	24.959565
149.569361	4743.381982	24.964583
149.692531	4739.411473	24.969600
149.381657	4747.918642	24.974618
149.828836	4727.562785	24.979635
150.005412	4729.027126	24.984653
149.937924	4729.977033	24.989671
150.280948	4727.290761	24.994688
149.868598	4752.597327	24.999706
150.522972	4753.026752	25.004723
150.195107	4748.647661	25.009741
150.194340	4768.696917	25.014759
150.497289	4775.015525	25.019776
150.828192	4784.789996	25.024794
150.919857	4793.440929	25.029811
150.919518	4801.028644	25.034829
151.292839	4817.084767	25.039847
151.637009	4823.999778	25.044864
151.431182	4820.028487	25.049882
151.898402	4826.777092	25.054899
151.666441	4846.119712	25.059917
151.818102	4844.795060	25.064935
152.243173	4838.790636	25.069952
152.099174	4846.486762	25.074970
152.836295	4845.578010	25.079987
152.918205	4868.052891	25.085005
152.907360	4870.010453	25.090023
153.218098	4862.141305	25.095040
153.134362	4871.266965	25.100058
153.341738	4868.208958	25.105075
153.344502	4862.475894	25.110093
153.465556	4890.607367	25.115111
153.717339	4882.518797	25.120128
153.506160	4888.727111	25.125146
153.961698	4895.147336	25.130163
154.518074	4915.428371	25.135181
154.661744	4922.543102	25.140199
154.783789	4912.941187	25.145216
154.581781	4927.438025	25.150234
154.893035	4909.373864	25.155251
155.048142	4927.412373	25.160269
154.896448	4945.965807	25.165287
155.233653	4940.938933	25.170304
154.826095	4952.263201	25.175322
155.323157	4955.632249	25.180339
155.497400	4978.996044	25.185357
155.618342	4982.079184	25.190375
156.158629	4989.874539	25.195392
155.914774	5014.140609	25.200410
156.369534	5014.088809	25.205427
156.390313	5016.018328	25.210445
156.427438	5029.893416	25.215463
156.564840	5034.376724	25.220480
156.868917	5039.642013	25.225498
156.935967	5053.509422	25.230515
157.383159	5056.786724	25.235533
157.296056	5058.720686	25.240551
157.684299	5055.702056	25.245568
157.977654	5088.390071	25.250586
157.706247	5095.976651	25.255603
158.064902	5097.725144	25.260621
158.012280	5094.341516	25.265639
158.479800	5103.377802	25.270656
158.209181	5124.934835	25.275674
158.637609	5115.464077	25.280691
158.973586	5128.271276	25.285709
158.924247	5151.041110	25.290727
159.378662	5138.435437	25.295744
159.577025	5144.575001	25.300762
159.804738	5148.068132	25.305779
159.983293	5164.427687	25.310797
159.927252	5177.876920	25.315815
160.367638	5180.785653	25.320832
160.280050	5172.914441	25.325850
160.256931	5167.928920	25.330867
160.693937	5166.222416	25.335885
160.701427	5194.671261	25.340903
161.112857	5200.271262	25.345920
161.130312	5190.317131	25.350938
160.864638	5189.209059	25.355955
161.033600	5208.133878	25.360973
161.401403	5220.934319	25.365991
162.061449	5222.094786	25.371008
161.713657	5218.663042	25.376026
162.046549	5219.232619	25.381043
162.049917	5243.872018	25.386061
162.159926	5251.555904	25.391079
162.342363	5250.384810	25.396096
162.238336	5266.782107	25.401114
162.315654	5276.270802	25.406131
162.682801	5280.650859	25.411149
162.749139	5281.712953	25.416167
163.504242	5294.973138	25.421184
163.486823	5311.200643	25.426202
163.944749	5292.175489	25.431219
163.920641	5297.467529	25.436237
163.765540	5299.940370	25.441255
164.129507	5287.434571	25.446272
164.455870	5313.068061	25.451290
164.453545	5316.802410	25.456307
164.900432	5330.788426	25.461325
165.088956	5328.859942	25.466343
164.858321	5326.374666	25.471360
164.635577	5329.811150	25.476378
164.805713	5335.788114	25.481395
164.951740	5349.243087	25.486413
164.899266	5360.797591	25.491431
165.216980	5366.655290	25.496448
165.353837	5388.097714	25.501466
165.020178	5404.905579	25.506483
165.755611	5417.016236	25.511501
166.098229	5432.871745	25.516519
166.258161	5446.172125	25.521536
166.520314	5449.697039	25.526554
166.536244	5453.547316	25.531571
166.771654	5466.622619	25.536589
166.608932	5479.681817	25.541607
167.128890	5478.104505	25.546624
167.332843	5492.550145	25.551642
167.831829	5506.949413	25.556659
168.300204	5504.037158	25.561677
168.182120	5512.035664	25.566695
168.287887	5526.153030	25.571712
168.575115	5530.002204	25.576730
168.635215	5535.252456	25.581747
169.383209	5522.288482	25.586765
168.880428	5530.018631	25.591783
169.251421	5535.618349	25.596800
169.401256	5557.037598	25.601818
169.432097	5558.727697	25.606835
169.494492	5556.670008	25.611853
169.368034	5564.744736	25.616871
169.727700	5580.483393	25.621888
169.739944	5593.750813	25.626906
170.087341	5595.195675	25.631923
170.035143	5618.781722	25.636941
170.107088	5611.990760	25.641959
170.888634	5634.883886	25.646976
170.761046	5644.829154	25.651994
171.030582	5646.916100	25.657011
171.447452	5641.437597	25.662029
171.345685	5654.403394	25.667047
171.730821	5662.527124	25.672064
171.723783	5676.115556	25.677082
171.978034	5675.023917	25.682100
172.323685	5674.172326	25.687117
172.207623	5696.025118	25.692135
172.385019	5710.012296	25.697152
172.717154	5702.023036	25.702170
172.692963	5704.884206	25.707188
173.402011	5708.653885	25.712205
173.340115	5732.883521	25.717223
173.501007	5715.367362	25.722240
173.654687	5718.673615	25.727258
173.179871	5716.100258	25.732276
173.476047	5726.678408	25.737293
173.520523	5742.832740	25.742311
173.928158	5762.211773	25.747328
174.089989	5772.167971	25.752346
174.202231	5778.395647	25.757364
174.604179	5791.388974	25.762381
174.513990	5807.721549	25.767399
175.084180	5808.137360	25.772416
175.040958	5820.355725	25.777434
174.797918	5823.075492	25.782452
175.374251	5824.401437	25.787469
175.272706	5836.706627	25.792487
175.617436	5855.301178	25.797504
175.810266	5857.721342	25.802522
176.089932	5854.529531	25.807540
176.228792	5873.750721	25.812557
176.878106	5886.311468	25.817575
176.865685	5894.645909	25.822592
177.034167	5891.496480	25.827610
176.895319	5888.323018	25.832628
177.556174	5907.827345	25.837645
177.560752	5918.821968	25.842663
177.717425	5932.607227	25.847680
177.904577	5924.318142	25.852698
178.143520	5928.713660	25.857716
178.040351	5937.251728	25.862733
178.136413	5955.388987	25.867751
178.421239	5960.507355	25.872768
178.417969	5958.649467	25.877786
178.652986	5982.564250	25.882804
178.851743	5989.259282	25.887821
179.214307	6005.429448	25.892839
179.381495	6015.416810	25.897856
179.538549	6013.621415	25.902874
179.363332	6031.226333	25.907892
179.667581	6043.158292	25.912909
180.032914	6052.420708	25.917927
180.431932	6061.573612	25.922944
180.662977	6062.295505	25.927962
180.580388	6069.823004	25.932980
181.328456	6058.105623	25.937997
180.993484	6076.696976	25.943015
181.180724	6088.075773	25.948032
181.875967	6087.752317	25.953050
181.768397	6092.259080	25.958068
181.986742	6092.909834	25.963085
182.025845	6112.100153	25.968103
181.968570	6124.856593	25.973120
182.127951	6128.158448	25.978138
182.078835	6136.215178	25.983156
182.910685	6146.036890	25.988173
182.789709	6165.427767	25.993191
182.847735	6170.634079	25.998208
183.161103	6173.230865	26.003226
183.094696	6185.613213	26.008244
183.255335	6201.539735	26.013261
183.619471	6211.829381	26.018279
183.925620	6210.358205	26.023296
183.960979	6232.029218	26.028314
183.827227	6234.217922	26.033332
184.193049	6263.028465	26.038349
184.283491	6278.989502	26.043367
184.555647	6284.163622	26.048384
184.944046	6295.372302	26.053402
185.229757	6299.169942	26.058420
185.435906	6298.189376	26.063437
185.706921	6314.834120	26.068455
186.177578	6312.211943	26.073472
186.539309	6317.054685	26.078490
186.679715	6321.495340	26.083508
187.102112	6315.205714	26.088525
187.086044	6314.536712	26.093543
187.128197	6313.302880	26.098560
187.254898	6305.939878	26.103578
187.090863	6323.831513	26.108596
187.633079	6328.858648	26.113613
187.703609	6340.189184	26.118631
187.541770	6349.166375	26.123648
188.142187	6335.300374	26.128666
188.168743	6357.858993	26.133684
188.553516	6341.047005	26.138701
188.373510	6361.583503	26.143719
188.184046	6372.183659	26.148736
188.373863	6373.763707	26.153754
188.407231	6386.959005	26.158772
188.698094	6399.721937	26.163789
188.956198	6418.693737	26.168807
188.954471	6446.267481	26.173824
189.137813	6447.760402	26.178842
189.614492	6470.034536	26.183860
189.931273	6474.343712	26.188877
189.914150	6478.626156	26.193895
190.328234	6504.103377	26.198912
190.796784	6503.254278	26.203930
190.640436	6522.108034	26.208948
190.840223	6542.433958	26.213965
190.890859	6541.280610	26.218983
191.633519	6546.607041	26.224000
191.779232	6552.592051	26.229018
191.480276	6566.553561	26.234036
191.948597	6569.570563	26.239053
192.146151	6580.667648	26.244071
192.056760	6585.241640	26.249088
192.579074	6602.565774	26.254106
192.598495	6615.500526	26.259124
193.087751	6619.372509	26.264141
193.451789	6631.120989	26.269159
193.746543	6647.581027	26.274176
193.581571	6638.945340	26.279194
193.693563	6638.387474	26.284212
193.852576	6645.458715	26.289229
194.005609	6664.782095	26.294247
194.058797	6672.217356	26.299264
194.416311	6686.669835	26.304282
194.109088	6705.645607	26.309300
194.815867	6713.151673	26.314317
194.935288	6728.801233	26.319335
194.610883	6735.971289	26.324352
195.336492	6754.066096	26.329370
195.201978	6760.906304	26.334388
195.956790	6772.917162	26.339405
196.235546	6792.229376	26.344423
196.655070	6800.547665	26.349440
197.028017	6798.329820	26.354458
196.818601	6801.945559	26.359476
196.780306	6810.842745	26.364493
196.839076	6836.005909	26.369511
196.993724	6831.493738	26.374528
197.653791	6849.122223	26.379546
197.776151	6862.078760	26.384564
197.973154	6861.408396	26.389581
198.262359	6860.263649	26.394599
198.497622	6879.699716	26.399616
198.764917	6876.309311	26.404634
198.853024	6891.988622	26.409652
199.074203	6887.741877	26.414669
199.548884	6898.238167	26.419687
199.312594	6911.911618	26.424704
199.215551	6901.090886	26.429722
199.561491	6910.423172	26.434740
200.032673	6930.853607	26.439757
200.309412	6929.123392	26.444775
200.103700	6933.506424	26.449792
200.284333	6950.140786	26.454810
200.411579	6955.216998	26.459828
200.552083	6967.350768	26.464845
200.771894	6971.724934	26.469863
200.913353	6984.965092	26.474880
201.271895	6991.655418	26.479898
201.383874	6995.117289	26.484916
201.278760	7013.448885	26.489933
201.675769	7022.689317	26.494951
201.692288	7048.484344	26.499968
202.222772	7045.652909	26.504986
202.065167	7065.278553	26.510004
202.535396	7086.525272	26.515021
203.140204	7084.768401	26.520039
203.379927	7102.088587	26.525056
203.469288	7104.696552	26.530074
203.496322	7113.283838	26.535092
203.679770	7119.908639	26.540109
204.007084	7138.636752	26.545127
204.140038	7145.449475	26.550144
204.449561	7145.309448	26.555162
204.515540	7162.907281	26.560180
205.012028	7172.959109	26.565197
205.100617	7183.125593	26.570215
205.096320	7186.333429	26.575232
205.392507	7199.696267	26.580250
205.588777	7215.319437	26.585268
205.802742	7215.309398	26.590285
206.119273	7221.801205	26.595303
206.190140	7244.608161	26.600320
206.453018	7259.902188	26.605338
206.631493	7261.135302	26.610356
206.925303	7261.179803	26.615373
207.278738	7285.207349	26.620391
207.525166	7294.932770	26.625408
207.668926	7280.586149	26.630426
207.586928	7311.628218	26.635444
207.962367	7326.270494	26.640461
208.014119	7313.374025	26.645479
208.417452	7331.099814	26.650496
208.777167	7348.651686	26.655514
208.876552	7341.664455	26.660532
208.916771	7370.192951	26.665549
209.171433	7373.673862	26.670567
209.478675	7381.156480	26.675584
209.774631	7390.410675	26.680602
210.121240	7410.100719	26.685620
210.205980	7403.908195	26.690637
210.526086	7420.801967	26.695655
210.787579	7432.458516	26.700672
210.412756	7433.742107	26.705690
210.794867	7431.577794	26.710708
210.907087	7459.593648	26.715725
211.392044	7466.068756	26.720743
211.163870	7477.161205	26.725760
211.540358	7486.712463	26.730778
211.952128	7498.374948	26.735796
211.964454	7513.441261	26.740813
212.501121	7521.249909	26.745831
212.601831	7534.133392	26.750848
213.078936	7540.698039	26.755866
213.040734	7560.627483	26.760884
213.082759	7570.934227	26.765901
213.462576	7566.505934	26.770919
213.435650	7585.159216	26.775936
213.621844	7581.254371	26.780954
213.893100	7587.545885	26.785972
214.323968	7603.813527	26.790989
214.913967	7618.171745	26.796007
214.496454	7620.092483	26.801024
214.760912	7623.273331	26.806042
215.102183	7639.890544	26.811060
215.096226	7637.150789	26.816077
215.569175	7639.802580	26.821095
215.290882	7664.388737	26.826112
215.481513	7676.279278	26.831130
215.836450	7686.083889	26.836148
215.713955	7712.853605	26.841165
216.253285	7725.109514	26.846183
216.431198	7738.227716	26.851200
216.400617	7748.526093	26.856218
216.847226	7759.953823	26.861236
216.725435	7783.740091	26.866253
217.332583	7805.500732	26.871271
217.993471	7826.958747	26.876288
217.944176	7826.010844	26.881306
218.124966	7833.655552	26.886324
218.198193	7868.065303	26.891341
218.721636	7861.610303	26.896359
218.608431	7887.873134	26.901376
218.869499	7893.486744	26.906394
219.087335	7907.278201	26.911412
219.040354	7924.219773	26.916429
219.689046	7944.686781	26.921447
219.912485	7956.057800	26.926464
220.104712	7971.446891	26.931482
220.738711	7980.168286	26.936500
220.665021	7988.875080	26.941517
220.973364	8005.261045	26.946535
221.328438	8017.910718	26.951552
221.647601	8025.889449	26.956570
221.534948	8031.831858	26.961588
221.556084	8055.588618	26.966605
221.920049	8073.770692	26.971623
222.221347	8079.437582	26.976640
222.205168	8087.393775	26.981658
222.894439	8103.244331	26.986676
222.804980	8103.745973	26.991693
223.254833	8116.035086	26.996711
223.582260	8125.868932	27.001728
223.507072	8134.448458	27.006746
223.953324	8163.214535	27.011764
223.943325	8180.651201	27.016781
224.408157	8173.603226	27.021799
224.504555	8194.947861	27.026816
224.499614	8206.956179	27.031834
225.240458	8215.582078	27.036852
224.957339	8230.211132	27.041869
225.256462	8234.709595	27.046887
225.578302	8249.183582	27.051904
225.879271	8267.653533	27.056922
226.205962	8283.082146	27.061940
226.370869	8299.155796	27.066957
226.502823	8305.274493	27.071975
226.931419	8327.111039	27.076992
226.862239	8324.349318	27.082010
227.359875	8329.890131	27.087028
227.238004	8360.812460	27.092045
227.749006	8351.212714	27.097063
227.927113	8371.880111	27.102080
228.060874	8386.920891	27.107098
228.386639	8397.531792	27.112116
228.521174	8402.617507	27.117133
228.900493	8420.714742	27.122151
229.146694	8420.134642	27.127168
229.220565	8443.358703	27.132186
229.345357	8445.320685	27.137204
229.676299	8456.075696	27.142221
229.938457	8466.133201	27.147239
229.961049	8490.720547	27.152256
230.288079	8489.358351	27.157274
230.363722	8499.679048	27.162292
230.267918	8524.159196	27.167309
230.640177	8531.561520	27.172327
230.965098	8548.250128	27.177344
231.111627	8574.290811	27.182362
231.655367	8577.546221	27.187380
231.416235	8598.652256	27.192397
231.959788	8616.405158	27.197415
232.272986	8626.425189	27.202432
232.389496	8639.662980	27.207450
232.757037	8650.228553	27.212468
233.155286	8676.230965	27.217485
233.682764	8656.706269	27.222503
233.796994	8663.338431	27.227520
233.916975	8685.851068	27.232538
234.289577	8683.323479	27.237556
234.584869	8695.889054	27.242573
234.998189	8719.982929	27.247591
235.116270	8708.963947	27.252608
235.219569	8720.821656	27.257626
235.521357	8733.127838	27.262644
235.674321	8743.676941	27.267661
235.894092	8744.828525	27.272679
236.286115	8773.568440	27.277696
236.271060	8784.452516	27.282714
236.664889	8777.239572	27.287732
236.387897	8792.778662	27.292749
236.405361	8814.756272	27.297767
236.803267	8824.203984	27.302784
236.736129	8855.711341	27.307802
237.349987	8878.278919	27.312820
237.609036	8894.023342	27.317837
237.953726	8920.704517	27.322855
238.420266	8930.290609	27.327872
238.315025	8947.024715	27.332890
238.604657	8954.442465	27.337908
239.164838	8982.809979	27.342925
239.389401	8984.214418	27.347943
239.512594	9001.707959	27.352960
240.035389	9007.673348	27.357978
240.040403	9007.634034	27.362996
240.213469	9046.341541	27.368013
240.388849	9048.644967	27.373031
240.692395	9058.622758	27.378048
240.839207	9077.701213	27.383066
240.982473	9088.098551	27.388084
241.244448	9102.452456	27.393101
241.531588	9119.403115	27.398119
242.018976	9130.474588	27.403136
242.120660	9152.612038	27.408154
242.526504	9164.905302	27.413172
242.374448	9178.146166	27.418189
242.836108	9195.945545	27.423207
243.306129	9210.818912	27.428224
243.461630	9221.686137	27.433242
243.887484	9227.622728	27.438260
243.996306	9241.502673	27.443277
244.201986	9256.035369	27.448295
244.499651	9265.670834	27.453312
244.233508	9275.612129	27.458330
244.601683	9289.889581	27.463348
244.953926	9307.705588	27.468365
244.958999	9329.295265	27.473383
245.322460	9340.496060	27.478400
244.926943	9362.315805	27.483418
245.324068	9387.032490	27.488436
245.569057	9402.218118	27.493453
245.954471	9426.474427	27.498471
246.497088	9440.448290	27.503488
246.604077	9466.051923	27.508506
247.179093	9463.360802	27.513524
247.204753	9498.319150	27.518541
247.401633	9514.851912	27.523559
247.906440	9523.036250	27.528576
248.011314	9536.672920	27.533594
248.488723	9556.507079	27.538612
248.728338	9558.281663	27.543629
248.975769	9582.553917	27.548647
249.233855	9583.974140	27.553664
249.340141	9593.236547	27.558682
249.750888	9604.357248	27.563700
250.111578	9617.376704	27.568717
250.363519	9644.242198	27.573735
250.681332	9642.851499	27.578752
250.512213	9670.275764	27.583770
251.179720	9668.653205	27.588788
251.117709	9675.776501	27.593805
251.328934	9701.407401	27.598823
252.242296	9708.997363	27.603840
251.883944	9729.423536	27.608858
252.472749	9734.455107	27.613876
252.350919	9744.211370	27.618893
252.374253	9776.306618	27.623911
253.103899	9782.283026	27.628928
253.050666	9818.429580	27.633946
253.193784	9830.185438	27.638964
253.448109	9839.070636	27.643981
253.799637	9874.769981	27.648999
254.050488	9879.496662	27.654016
254.312966	9915.480996	27.659034
254.546448	9931.992390	27.664052
254.875119	9940.995334	27.669069
255.102836	9951.068925	27.674087
255.581989	9964.298319	27.679104
255.640318	9990.329897	27.684122
256.129346	9994.029465	27.689140
256.359521	10023.382078	27.694157
256.542365	10038.999224	27.699175
256.741777	10045.644672	27.704192
257.055234	10079.623297	27.709210
257.090785	10078.036578	27.714228
257.631456	10097.410384	27.719245
257.386952	10123.727740	27.724263
258.049049	10120.920510	27.729280
258.010352	10155.326132	27.734298
258.526915	10173.698877	27.739316
259.148505	10192.181903	27.744333
258.866239	10204.157197	27.749351
259.458508	10214.521264	27.754368
259.381695	10238.796885	27.759386
259.658978	10259.390483	27.764404
260.427614	10259.527493	27.769421
260.338949	10291.058571	27.774439
260.707727	10296.172363	27.779456
260.659039	10321.915734	27.784474
261.135831	10331.719973	27.789492
261.638556	10352.385940	27.794509
261.149342	10382.426810	27.799527
261.665592	10386.593040	27.804544
262.032764	10403.568081	27.809562
262.046704	10422.268352	27.814580
262.648541	10442.591150	27.819597
262.613134	10457.316019	27.824615
263.047020	10472.080741	27.829632
263.239579	10499.664090	27.834650
263.435986	10514.709135	27.839668
263.870154	10532.245933	27.844685
263.791281	10539.833228	27.849703
264.357508	10551.507110	27.854720
264.535876	10583.025367	27.859738
265.143389	10596.037931	27.864756
265.396814	10602.323353	27.869773
265.652058	10620.227752	27.874791
266.170153	10630.724872	27.879808
266.264791	10648.708616	27.884826
266.311840	10657.815212	27.889844
267.064882	10674.279349	27.894861
266.846202	10687.006251	27.899879
267.220504	10699.585567	27.904896
267.435875	10731.106667	27.909914
267.942371	10739.541075	27.914932
268.237699	10752.302847	27.919949
267.808361	10783.118389	27.924967
268.757218	10788.659574	27.929984
268.959889	10807.001407	27.935002
269.142633	10813.527827	27.940020
269.903202	10826.752409	27.945037
270.001336	10841.839207	27.950055
270.286941	10847.616819	27.955072
270.189033	10868.387414	27.960090
270.558697	10878.420810	27.965108
270.908711	10910.082297	27.970125
271.105973	10917.456357	27.975143
271.515223	10929.811082	27.980160
271.758437	10941.997883	27.985178
271.903824	10958.647785	27.990196
272.261758	10963.298804	27.995213
272.377031	10987.240534	28.000231
272.761930	10996.561711	28.005248
273.094935	11008.318575	28.010266
273.085087	11029.040955	28.015284
273.639283	11046.531705	28.020301
273.452988	11070.398127	28.025319
273.775923	11080.162863	28.030336
274.372484	11099.598766	28.035354
274.441353	11132.993761	28.040372
274.553305	11141.365159	28.045389
274.637947	11180.413072	28.050407
274.984667	11190.723813	28.055424
275.183685	11215.890432	28.060442
275.645326	11246.638441	28.065460
276.040003	11263.358550	28.070477
276.088121	11289.220615	28.075495
276.703521	11310.476587	28.080512
276.976394	11320.066187	28.085530
276.949962	11334.128641	28.090548
277.958906	11352.697911	28.095565
278.069983	11368.309305	28.100583
278.552982	11377.890222	28.105600
278.875261	11398.087900	28.110618
278.847282	11413.375686	28.115636
279.394529	11422.416622	28.120653
279.554039	11439.245093	28.125671
279.953192	11449.518191	28.130688
280.439852	11465.859357	28.135706
280.244317	11485.983561	28.140724
280.609548	11491.907386	28.145741
280.443997	11509.729469	28.150759
280.766278	11519.228308	28.155776
280.989811	11541.128354	28.160794
280.668588	11569.104090	28.165812
280.957218	11579.590904	28.170829
281.068342	11616.379257	28.175847
281.591343	11642.521095	28.180864
282.143328	11665.163511	28.185882
282.516032	11679.099664	28.190900
283.024614	11703.612451	28.195917
283.014410	11730.145039	28.200935
283.665813	11725.325686	28.205952
284.412253	11753.191528	28.210970
284.422739	11762.912977	28.215988
284.979222	11772.206259	28.221005
285.040162	11788.230489	28.226023
285.196591	11804.941681	28.231040
285.394747	11818.497134	28.236058
285.393322	11838.597587	28.241076
286.092962	11852.559448	28.246093
286.201041	11872.242433	28.251111
286.400154	11898.724961	28.256128
286.582702	11917.559043	28.261146
286.755338	11944.063352	28.266164
287.543422	11966.522230	28.271181
287.251860	11981.009566	28.276199
287.691841	11997.662296	28.281216
288.452597	12017.443249	28.286234
288.504628	12036.105231	28.291252
288.967792	12052.783338	28.296269
289.208484	12080.812085	28.301287
289.680973	12091.988926	28.306304
290.184179	12107.748967	28.311322
289.865514	12137.733421	28.316340
290.575421	12146.551729	28.321357
290.728204	12167.518142	28.326375
290.650089	12180.489285	28.331392
291.176670	12204.449175	28.336410
291.061428	12217.758943	28.341428
291.582813	12239.369658	28.346445
291.919105	12261.219756	28.351463
292.189469	12279.285015	28.356480
292.289913	12309.265148	28.361498
292.441809	12343.240599	28.366516
293.007947	12353.760856	28.371533
293.117910	12388.490196	28.376551
293.141206	12407.559938	28.381568
293.595166	12437.243191	28.386586
294.006114	12472.830574	28.391604
294.684568	12489.553927	28.396621
295.121335	12502.480444	28.401639
295.710699	12530.223897	28.406656
295.927284	12530.891767	28.411674
296.483681	12546.604848	28.416692
296.664998	12564.925431	28.421709
296.692851	12574.696498	28.426727
296.930294	12596.482234	28.431744
297.472700	12607.039668	28.436762
297.545951	12631.417800	28.441780
297.647994	12649.075603	28.446797
298.003524	12667.679509	28.451815
298.101142	12695.876352	28.456832
298.770874	12710.662479	28.461850
298.426588	12738.705502	28.466868
298.985401	12748.374774	28.471885
299.396649	12767.872468	28.476903
299.549341	12788.352023	28.481920
299.989384	12811.191817	28.486938
300.174142	12833.731888	28.491956
300.640766	12843.618139	28.496973
300.706647	12866.385889	28.501991
300.945588	12884.954157	28.507008
301.668269	12900.371453	28.512026
301.778455	12925.985594	28.517044
301.763859	12935.689833	28.522061
302.197412	12957.029242	28.527079
302.749583	12977.420981	28.532096
303.538657	12984.277501	28.537114
303.251497	13002.278893	28.542132
303.612052	13028.144919	28.547149
304.144403	13044.703112	28.552167
303.966989	13065.770153	28.557184
304.452877	13079.077439	28.562202
304.695283	13113.172707	28.567220
305.000905	13119.548192	28.572237
305.357352	13149.088141	28.577255
305.191725	13173.382072	28.582272
305.734326	13186.401170	28.587290
305.905969	13224.028580	28.592308
306.451663	13238.914474	28.597325
306.480617	13275.457823	28.602343
306.896172	13295.488050	28.607360
307.573704	13313.049928	28.612378
307.910359	13341.592892	28.617396
308.004535	13368.305533	28.622413
308.189277	13391.522387	28.627431
308.607795	13408.348732	28.632448
309.490869	13435.148608	28.637466
309.146223	13456.834698	28.642484
309.972244	13479.176758	28.647501
310.262096	13504.027821	28.652519
310.297351	13529.587539	28.657536
310.772844	13527.518885	28.662554
310.827463	13567.835798	28.667572
311.049716	13593.657819	28.672589
311.287538	13605.796318	28.677607
311.680586	13633.265248	28.682624
312.425536	13647.608045	28.687642
312.025473	13683.110681	28.692660
313.131998	13696.673650	28.697677
313.169844	13723.422971	28.702695
313.474017	13752.146939	28.707712
314.048482	13757.671453	28.712730
314.324715	13785.593285	28.717748
314.709185	13812.331187	28.722765
315.070375	13824.492016	28.727783
315.372603	13832.363788	28.732800
315.975554	13844.587120	28.737818
316.445228	13863.981938	28.742836
316.578364	13877.368646	28.747853
317.076047	13883.726888	28.752871
317.180378	13915.514451	28.757888
317.417748	13919.244702	28.762906
317.544372	13938.664768	28.767924
317.780305	13952.880770	28.772941
318.283143	13971.086797	28.777959
318.412810	13988.613856	28.782976
318.671729	14013.382566	28.787994
318.632831	14044.886758	28.793012
319.429507	14059.834377	28.798029
319.718075	14086.497176	28.803047
319.389832	14112.379452	28.808064
319.942710	14135.623225	28.813082
320.300974	14160.383626	28.818100
320.594559	14176.731869	28.823117
321.000891	14208.555209	28.828135
321.110753	14232.286758	28.833152
321.420533	14239.276581	28.838170
321.526331	14274.438497	28.843188
321.963079	14288.301720	28.848205
322.157530	14324.635716	28.853223
322.174923	14360.488465	28.858240
322.791438	14359.868266	28.863258
323.602720	14376.523574	28.868276
324.386796	14399.893423	28.873293
324.581707	14422.911515	28.878311
324.666958	14446.067523	28.883328
325.496320	14455.954723	28.888346
325.815692	14478.145487	28.893364
325.889939	14501.836037	28.898381
326.205066	14504.574960	28.903399
326.153028	14529.783494	28.908416
326.740948	14553.814745	28.913434
326.611765	14566.482631	28.918452
326.778995	14596.934245	28.923469
327.300494	14625.735744	28.928487
327.261717	14655.937842	28.933504
328.014509	14674.004085	28.938522
328.197396	14723.077235	28.943540
328.149942	14759.236268	28.948557
328.489377	14775.323819	28.953575
328.770947	14812.774433	28.958592
329.220817	14855.361581	28.963610
329.341624	14880.255286	28.968628
330.192372	14902.836346	28.973645
330.700694	14921.740665	28.978663
331.457731	14953.212830	28.983680
332.142627	14957.536003	28.988698
332.147571	14980.614633	28.993716
332.230735	15018.284456	28.998733
333.053359	15024.217551	29.003751
333.111340	15044.597408	29.008768
333.235004	15058.295535	29.013786
333.493050	15083.625474	29.018804
333.729725	15114.329762	29.023821
333.863332	15136.933490	29.028839
334.117102	15169.222025	29.033856
334.523592	15194.306981	29.038874
334.980667	15225.362749	29.043892
335.215020	15265.822803	29.048909
335.447217	15286.218307	29.053927
335.678284	15319.513193	29.058944
336.266009	15332.707804	29.063962
336.951642	15366.465092	29.068980
337.388425	15401.751267	29.073997
337.834240	15424.472444	29.079015
338.047263	15458.905290	29.084032
338.522500	15474.763071	29.089050
338.431823	15488.199110	29.094068
338.577600	15522.091609	29.099085
339.332624	15547.244032	29.104103
339.407633	15569.791848	29.109120
339.734924	15592.810212	29.114138
340.379614	15614.956663	29.119156
340.738128	15647.399045	29.124173
340.792524	15674.013300	29.129191
341.163050	15701.520966	29.134208
341.276214	15735.293215	29.139226
341.787223	15760.885006	29.144244
342.222275	15783.792853	29.149261
342.747115	15805.693019	29.154279
343.005581	15838.399741	29.159296
343.261401	15858.497345	29.164314
343.854421	15881.448577	29.169332
343.901128	15895.265712	29.174349
344.479137	15914.917733	29.179367
344.597215	15933.897153	29.184384
344.999027	15955.564107	29.189402
345.400853	15976.252381	29.194420
345.545128	16014.027875	29.199437
345.949268	16025.619045	29.204455
346.493685	16041.845771	29.209472
346.606154	16076.357994	29.214490
347.119688	16086.484343	29.219508
347.010726	16111.797705	29.224525
347.594186	16131.997546	29.229543
347.718375	16169.048590	29.234560
348.105111	16196.630062	29.239578
348.423888	16226.982453	29.244596
348.424882	16265.637988	29.249613
348.900805	16300.158408	29.254631
349.268052	16331.703935	29.259648
349.437614	16368.409083	29.264666
350.076563	16407.623080	29.269684
350.315506	16441.002479	29.274701
350.787644	16463.049351	29.279719
350.941876	16508.759819	29.284736
351.405119	16539.013272	29.289754
352.237040	16558.493308	29.294772
352.097224	16598.269833	29.299789
352.804595	16620.768217	29.304807
353.156787	16650.208051	29.309824
353.535987	16686.671235	29.314842
353.808624	16708.481884	29.319860
353.975154	16749.628221	29.324877
354.464630	16780.580723	29.329895
355.047671	16804.171641	29.334912
355.524583	16833.228698	29.339930
355.936769	16861.593558	29.344948
356.240982	16888.466396	29.349965
356.560254	16913.139699	29.354983
356.896965	16947.350345	29.360000
357.294845	16977.418391	29.365018
357.702433	17006.684221	29.370036
357.826629	17034.628849	29.375053
358.066901	17057.384675	29.380071
358.655838	17097.473875	29.385088
358.849205	17132.487192	29.390106
359.599302	17156.296896	29.395124
359.860798	17181.899030	29.400141
360.178185	17196.815240	29.405159
360.585322	17230.770542	29.410176
360.698755	17255.049653	29.415194
361.325853	17280.164410	29.420212
361.567039	17320.882166	29.425229
361.998421	17343.359361	29.430247
362.544055	17369.329375	29.435264
362.709410	17397.089714	29.440282
363.312046	17421.721698	29.445300
363.423460	17463.287149	29.450317
363.640220	17477.090131	29.455335
364.367287	17501.626023	29.460352
364.592326	17531.335899	29.465370
364.786328	17557.088470	29.470388
364.897489	17586.252989	29.475405
365.387599	17615.974394	29.480423
365.836080	17653.315663	29.485440
366.169741	17683.546922	29.490458
366.670406	17705.114744	29.495476
367.106133	17739.408404	29.500493
367.510907	17762.907209	29.505511
368.047443	17792.782035	29.510528
367.888550	17827.565003	29.515546
368.311407	17833.896182	29.520564
368.604804	17861.850514	29.525581
369.078685	17885.013379	29.530599
369.473076	17914.820490	29.535616
369.558758	17954.786856	29.540634
370.042834	17979.927886	29.545652
370.019788	18012.179477	29.550669
370.311374	18042.243384	29.555687
370.851521	18092.873758	29.560704
370.904159	18123.130180	29.565722
371.597326	18156.565696	29.570740
371.872872	18205.823101	29.575757
372.424815	18236.351898	29.580775
372.899404	18271.086317	29.585792
373.249853	18300.039181	29.590810
374.072583	18327.381970	29.595828
374.307313	18352.498557	29.600845
375.095179	18376.732530	29.605863
375.260271	18403.632399	29.610880
375.872421	18416.957875	29.615898
376.441875	18432.962160	29.620916
376.696174	18461.521366	29.625933
377.220945	18477.462145	29.630951
377.885356	18503.360735	29.635968
377.579160	18534.031843	29.640986
378.062950	18546.536905	29.646004
378.298459	18575.756714	29.651021
378.556708	18612.080209	29.656039
378.857636	18634.248125	29.661056
379.110829	18665.607322	29.666074
379.784525	18695.831551	29.671092
380.125286	18730.054685	29.676109
380.549688	18763.663510	29.681127
381.057210	18792.651188	29.686144
381.021762	18827.389065	29.691162
381.715493	18844.052601	29.696180
382.056144	18883.884514	29.701197
382.438908	18911.537397	29.706215
382.724120	18942.824049	29.711232
382.591592	18977.439563	29.716250
382.758729	19020.914931	29.721268
383.596380	19053.215523	29.726285
383.510802	19083.509141	29.731303
384.434574	19123.272098	29.736320
384.911720	19177.043611	29.741338
385.263699	19198.604846	29.746356
385.592202	19238.792715	29.751373
386.078346	19273.341323	29.756391
386.608859	19304.925470	29.761408
386.950392	19334.485353	29.766426
387.508408	19365.962612	29.771444
387.899479	19400.710046	29.776461
388.205907	19418.727592	29.781479
388.648191	19465.716483	29.786496
388.907604	19490.712492	29.791514
389.662673	19508.799471	29.796532
389.889505	19546.719168	29.801549
389.826332	19571.833218	29.806567
390.570343	19601.886698	29.811584
390.820510	19646.171272	29.816602
390.885917	19672.760206	29.821620
391.197634	19700.834421	29.826637
391.859549	19739.075200	29.831655
392.517334	19777.983558	29.836672
393.080837	19805.970643	29.841690
393.579454	19836.523812	29.846708
393.869326	19862.057624	29.851725
394.569761	19872.163323	29.856743
394.835063	19907.753893	29.861760
395.234707	19915.473783	29.866778
395.893705	19936.739343	29.871796
395.798281	19963.719457	29.876813
395.723621	19984.975433	29.881831
396.780008	20003.906997	29.886848
396.742076	20045.284474	29.891866
397.510134	20052.379217	29.896884
397.838955	20086.050648	29.901901
397.703077	20116.934574	29.906919
398.137481	20150.327010	29.911936
398.276677	20189.167509	29.916954
398.702374	20210.017951	29.921972
398.978648	20240.824563	29.926989
399.419080	20294.022477	29.932007
400.135705	20337.981183	29.937024
399.915985	20376.165707	29.942042
400.255785	20408.235894	29.947060
401.015125	20461.015927	29.952077
401.398282	20498.054380	29.957095
401.832363	20527.635777	29.962112
402.005520	20586.163035	29.967130
402.574091	20617.073396	29.972148
403.183906	20668.622349	29.977165
403.347190	20697.350196	29.982183
403.975676	20720.614454	29.987200
404.159434	20778.749670	29.992218
405.057185	20812.878776	29.997236
405.228682	20844.351742	30.002253
405.603767	20881.967796	30.007271
406.019610	20933.125534	30.012288
406.640192	20965.024288	30.017306
407.046049	21009.895289	30.022324
407.293905	21039.180445	30.027341
407.665214	21080.606389	30.032359
408.077509	21115.085888	30.037376
408.341480	21165.519008	30.042394
408.889785	21200.152784	30.047412
409.665001	21244.927141	30.052429
409.744160	21282.667076	30.057447
410.055748	21311.634759	30.062464
410.248135	21359.584651	30.067482
410.894938	21400.540215	30.072500
411.999204	21429.891109	30.077517
412.409839	21460.349855	30.082535
413.304057	21477.200486	30.087552
413.683366	21509.884264	30.092570
414.178797	21538.008474	30.097588
414.465986	21561.271951	30.102605
414.659814	21586.904671	30.107623
415.109739	21616.835374	30.112640
415.291813	21653.562763	30.117658
415.957843	21677.887906	30.122676
416.447050	21701.383068	30.127693
416.298376	21741.244307	30.132711
417.336516	21759.569186	30.137728
417.386565	21802.254480	30.142746
417.645668	21834.347038	30.147764
417.837586	21864.319226	30.152781
418.340730	21906.676111	30.157799
418.554302	21939.651393	30.162816
418.694709	21972.850089	30.167834
419.299160	22013.918204	30.172852
419.478098	22056.045234	30.177869
419.669542	22104.005292	30.182887
420.221927	22145.146969	30.187904
420.495808	22196.104981	30.192922
421.027052	22250.416655	30.197940
421.168620	22289.375146	30.202957
421.836908	22330.140239	30.207975
422.337878	22354.547237	30.212992
422.848014	22402.319911	30.218010
423.233899	22447.458200	30.223028
423.393410	22475.700961	30.228045
423.547853	22521.695953	30.233063
424.119734	22569.771076	30.238080
424.627807	22613.804898	30.243098
424.813855	22677.146087	30.248116
425.349636	22719.330925	30.253133
425.848194	22763.557485	30.258151
426.296184	22815.494519	30.263168
426.783340	22859.734252	30.268186
427.307958	22898.697096	30.273204
427.934513	22953.649613	30.278221
427.877434	23006.927279	30.283239
428.889587	23044.594304	30.288256
429.167778	23090.326018	30.293274
429.872502	23119.425809	30.298292
430.744858	23155.156346	30.303309
431.163116	23196.844637	30.308327
431.780899	23223.379489	30.313344
432.221510	23265.259767	30.318362
432.580634	23298.697715	30.323380
433.207429	23327.575810	30.328397
433.535704	23368.905709	30.333415
433.925139	23391.278174	30.338432
434.040684	23434.828705	30.343450
434.175359	23467.622920	30.348468
434.898578	23505.187339	30.353485
435.137752	23551.852287	30.358503
435.729097	23584.093541	30.363520
436.468662	23627.122077	30.368538
436.806981	23659.799457	30.373556
437.053767	23695.576137	30.378573
437.093444	23740.398230	30.383591
437.695730	23772.701108	30.388608
438.340415	23818.634416	30.393626
438.483871	23867.870395	30.398644
438.967226	23906.574332	30.403661
439.181693	23952.150189	30.408679
439.654050	23997.606306	30.413696
440.109095	24049.309450	30.418714
440.357587	24117.366595	30.423732
440.864836	24144.660666	30.428749
441.322703	24203.285915	30.433767
441.895809	24259.039901	30.438784
442.154872	24306.127799	30.443802
442.595709	24355.065356	30.448820
443.125524	24400.625015	30.453837
443.337655	24451.188478	30.458855
443.920268	24498.146198	30.463872
444.403485	24552.435362	30.468890
444.431112	24610.082918	30.473908
445.633351	24655.718254	30.478925
445.681384	24718.266765	30.483943
446.041932	24752.953053	30.488960
446.793464	24810.063844	30.493978
446.928848	24863.708183	30.498996
447.771804	24897.755297	30.504013
448.188496	24953.878002	30.509031
448.631159	24997.356430	30.514048
449.097586	25056.161393	30.519066
449.701543	25104.870747	30.524084
450.182406	25142.447293	30.529101
450.077224	25186.571762	30.534119
450.788085	25232.578388	30.539136
451.446015	25275.315521	30.544154
451.795727	25326.601573	30.549172
452.537028	25359.278734	30.554189
452.326341	25412.944121	30.559207
453.013605	25455.541247	30.564224
453.528403	25500.243764	30.569242
453.845438	25532.284881	30.574260
454.851109	25576.665247	30.579277
454.935933	25617.698640	30.584295
455.283362	25664.778852	30.589312
455.635814	25696.574735	30.594330
456.060849	25758.000354	30.599348
456.520584	25812.906112	30.604365
457.243950	25853.762057	30.609383
457.476000	25902.962476	30.614400
458.140289	25951.300007	30.619418
458.559147	25987.393705	30.624436
459.548820	26040.547390	30.629453
459.722004	26089.710762	30.634471
460.257517	26119.370364	30.639488
460.981855	26161.018523	30.644506
461.014034	26203.304673	30.649524
461.440161	26246.308038	30.654541
461.612684	26305.911766	30.659559
462.120700	26341.262915	30.664576
462.825128	26388.942179	30.669594
463.192631	26453.771918	30.674612
463.621843	26497.226425	30.679629
463.975010	26549.076989	30.684647
464.465145	26600.337358	30.689664
465.044784	26659.436657	30.694682
465.678203	26700.542883	30.699700
466.611676	26742.482781	30.704717
467.097873	26792.205196	30.709735
467.275789	26833.093652	30.714752
467.665010	26871.430347	30.719770
468.003838	26932.068551	30.724788
468.724582	26962.263600	30.729805
468.859251	27010.628525	30.734823
469.632571	27064.641197	30.739840
470.803500	27090.034093	30.744858
470.854947	27142.633349	30.749876
471.392945	27176.262268	30.754893
471.745232	27215.880104	30.759911
471.931483	27270.056632	30.764928
472.599011	27315.978246	30.769946
473.008515	27359.107005	30.774964
473.409966	27408.842050	30.779981
473.796098	27447.404487	30.784999
474.353377	27484.620288	30.790016
474.888867	27526.384971	30.795034
475.824189	27576.000773	30.800052
476.093523	27615.134865	30.805069
476.426695	27666.777618	30.810087
476.723258	27710.717624	30.815104
477.673612	27752.767604	30.820122
477.723453	27792.291629	30.825140
478.033268	27838.387278	30.830157
478.409687	27884.326952	30.835175
479.030252	27938.752424	30.840192
479.047038	27992.375674	30.845210
479.728213	28041.337701	30.850228
480.003769	28086.408217	30.855245
480.402838	28147.617988	30.860263
480.881707	28201.632399	30.865280
481.206631	28252.675792	30.870298
481.504763	28327.999591	30.875316
482.300219	28372.398269	30.880333
482.805350	28420.377902	30.885351
482.972469	28484.854094	30.890368
483.905924	28531.772813	30.895386
483.876092	28588.058446	30.900404
484.392126	28648.796438	30.905421
484.787128	28704.349851	30.910439
485.338883	28756.391911	30.915456
485.839468	28810.795787	30.920474
486.222846	28868.613376	30.925492
486.675457	28934.132366	30.930509
487.199574	28995.113131	30.935527
487.598874	29061.439488	30.940544
488.253878	29116.844025	30.945562
488.784491	29184.944069	30.950580
489.515078	29239.396471	30.955597
489.947473	29298.614310	30.960615
490.902816	29348.739781	30.965632
491.568617	29393.563123	30.970650
491.511820	29450.398587	30.975668
492.307157	29505.610841	30.980685
493.081455	29560.397724	30.985703
493.467819	29605.081649	30.990720
494.022045	29660.785327	30.995738
494.546996	29718.301604	31.000756
495.010015	29757.853348	31.005773
495.287711	29809.801881	31.010791
495.470123	29865.845237	31.015808
496.268263	29922.440079	31.020826
496.618806	29975.664165	31.025844
497.089460	30033.247236	31.030861
497.617180	30091.543490	31.035879
498.162654	30144.215373	31.040896
498.973156	30202.894327	31.045914
499.407277	30275.213469	31.050932
500.011012	30317.358488	31.055949
500.362354	30385.221540	31.060967
500.339149	30432.587349	31.065984
501.697082	30483.536077	31.071002
501.889259	30547.031501	31.076020
502.301489	30600.704744	31.081037
502.980302	30646.841548	31.086055
503.292692	30704.632800	31.091072
503.961792	30749.815583	31.096090
504.006688	30815.405847	31.101108
504.759634	30870.960690	31.106125
504.912590	30935.662829	31.111143
505.645580	30988.508198	31.116160
506.535197	31055.344805	31.121178
506.696419	31122.721576	31.126196
507.291720	31173.530128	31.131213
507.953827	31237.653972	31.136231
507.864296	31300.413097	31.141248
509.005113	31343.860033	31.146266
509.485513	31415.529496	31.151284
509.942725	31458.827775	31.156301
510.657202	31514.965212	31.161319
510.800972	31580.478910	31.166336
511.788997	31627.829205	31.171354
512.106043	31681.313259	31.176372
512.458097	31746.222127	31.181389
513.114556	31797.501943	31.186407
513.234244	31868.633393	31.191424
514.116177	31914.544383	31.196442
514.703951	31977.121489	31.201460
514.892613	32037.811785	31.206477
515.008617	32089.733852	31.211495
515.688514	32147.109484	31.216512
516.226280	32204.840061	31.221530
516.344823	32271.953802	31.226548
516.896572	32332.335892	31.231565
517.623071	32400.542322	31.236583
518.020085	32458.139224	31.241600
518.752083	32514.182310	31.246618
519.063072	32593.504135	31.251636
519.477556	32646.874068	31.256653
520.391678	32704.058230	31.261671
520.683993	32765.926555	31.266688
521.624356	32813.436215	31.271706
522.240772	32870.414522	31.276724
522.660649	32931.145429	31.281741
523.579110	32983.701139	31.286759
523.918543	33039.299598	31.291776
524.499347	33086.257275	31.296794
525.236386	33149.905597	31.301812
525.296509	33212.119894	31.306829
525.859420	33257.080568	31.311847
526.114797	33332.537116	31.316864
526.894599	33380.519716	31.321882
527.668569	33436.224346	31.326900
528.418232	33483.647411	31.331917
529.046203	33535.637469	31.336935
528.919196	33611.653746	31.341952
529.878432	33662.800638	31.346970
530.350049	33714.122877	31.351988
530.963719	33778.033643	31.357005
531.662142	33827.924097	31.362023
531.446745	33886.516615	31.367040
532.421416	33951.576879	31.372058
532.452146	34005.856783	31.377076
533.319923	34062.980430	31.382093
534.220283	34124.017873	31.387111
534.870003	34182.288619	31.392128
535.236432	34241.019707	31.397146
535.681781	34295.048999	31.402164
536.643521	34350.943219	31.407181
537.090402	34399.617814	31.412199
537.128798	34471.883882	31.417216
537.796445	34513.889570	31.422234
538.192331	34582.878476	31.427252
538.955119	34646.171357	31.432269
539.542608	34697.164911	31.437287
539.836761	34768.146676	31.442304
541.031405	34808.463022	31.447322
541.413606	34864.599736	31.452340
542.168292	34926.752657	31.457357
542.564785	34969.719313	31.462375
542.559977	35037.211016	31.467392
543.378016	35093.781353	31.472410
543.810971	35159.266854	31.477428
544.395990	35215.311218	31.482445
545.042392	35274.832550	31.487463
545.507643	35328.991076	31.492480
545.872555	35389.581700	31.497498
546.136217	35457.343054	31.502516
546.585553	35527.620596	31.507533
547.499404	35586.893680	31.512551
547.874191	35658.449465	31.517568
548.106659	35717.317996	31.522586
548.851802	35796.219524	31.527604
549.501195	35862.119962	31.532621
549.623716	35923.096401	31.537639
549.925959	36001.052692	31.542656
550.561885	36064.163285	31.547674
550.806084	36142.546336	31.552692
551.240502	36223.609109	31.557709
551.878572	36295.480556	31.562727
552.576426	36369.576714	31.567744
553.070862	36447.234960	31.572762
553.885035	36512.466793	31.577780
554.440485	36575.930154	31.582797
554.816647	36647.350807	31.587815
555.501060	36716.391816	31.592832
556.058108	36783.043051	31.597850
557.000523	36863.447290	31.602868
557.365126	36932.870164	31.607885
558.331101	36985.590813	31.612903
558.745407	37074.597828	31.617920
559.175723	37127.988055	31.622938
559.989271	37196.936997	31.627956
560.696237	37265.764946	31.632973
561.244009	37322.497432	31.637991
561.781041	37376.943797	31.643008
562.491033	37450.000942	31.648026
562.898577	37507.988003	31.653044
563.145055	37581.191668	31.658061
563.938292	37643.982014	31.663079
564.309383	37712.081298	31.668096
564.853583	37781.446221	31.673114
565.463725	37856.834880	31.678132
565.664639	37930.113762	31.683149
566.487232	37998.691866	31.688167
566.705367	38074.524908	31.693184
567.441799	38151.241585	31.698202
568.085776	38224.347487	31.703220
568.678916	38302.634968	31.708237
569.618478	38366.675581	31.713255
570.180706	38446.360646	31.718272
570.997861	38516.974176	31.723290
571.506467	38573.095299	31.728308
571.811384	38645.473018	31.733325
572.553655	38710.339635	31.738343
572.949477	38786.929050	31.743360
573.662632	38857.033998	31.748378
574.365555	38922.962054	31.753396
574.985206	38997.924651	31.758413
575.864541	39053.578876	31.763431
576.161699	39122.522618	31.768448
576.856040	39190.110104	31.773466
577.215388	39263.409243	31.778484
577.777774	39327.215702	31.783501
578.547428	39387.604585	31.788519
579.351747	39453.088563	31.793536
579.361620	39527.156659	31.798554
580.391800	39593.705401	31.803572
580.722276	39675.716183	31.808589
581.664607	39737.112995	31.813607
582.429778	39799.681886	31.818624
583.058349	39869.340724	31.823642
583.809430	39928.623420	31.828660
583.799087	39979.550777	31.833677
584.494303	40032.100935	31.838695
585.196816	40110.889493	31.843712
586.010305	40181.895192	31.848730
586.350202	40245.811061	31.853748
586.542865	40313.716001	31.858765
587.051842	40371.594460	31.863783
587.541561	40453.853899	31.868800
587.791277	40538.703808	31.873818
588.624967	40604.411188	31.878836
589.296706	40674.640459	31.883853
589.870025	40757.319900	31.888871
590.168643	40830.818451	31.893888
590.560088	40896.189568	31.898906
591.324715	40978.055580	31.903924
591.907495	41055.213934	31.908941
592.690706	41108.131448	31.913959
593.233723	41177.045504	31.918976
593.950531	41256.802567	31.923994
594.860243	41322.929276	31.929012
595.301714	41383.262174	31.934029
595.862979	41442.467495	31.939047
596.215925	41520.098228	31.944064
596.629001	41592.570791	31.949082
597.233758	41664.150200	31.954100
597.768326	41750.530711	31.959117
598.865415	41818.320261	31.964135
599.338904	41893.060035	31.969152
599.398585	41977.780679	31.974170
599.970976	42045.439911	31.979188
600.495188	42129.920381	31.984205
601.155315	42206.941371	31.989223
601.869101	42297.736468	31.994240
602.377582	42385.895242	31.999258
603.142877	42455.156200	32.004276
603.319380	42558.946493	32.009293
604.143214	42641.476236	32.014311
604.756837	42725.597413	32.019328
605.070795	42807.435514	32.024346
605.861018	42893.526607	32.029364
606.648210	42985.657812	32.034381
607.092698	43069.483324	32.039399
607.789645	43171.751534	32.044416
608.328881	43259.922028	32.049434
609.243002	43334.064491	32.054452
609.959334	43421.701388	32.059469
610.439665	43511.900138	32.064487
611.163604	43588.499623	32.069504
611.485337	43679.227348	32.074522
612.176588	43768.707432	32.079540
612.893718	43860.118963	32.084557
613.946905	43933.925152	32.089575
614.235273	44018.071191	32.094592
614.807037	44108.535565	32.099610
615.158322	44188.915009	32.104628
615.889861	44280.446200	32.109645
616.509016	44376.908956	32.114663
617.576728	44457.237538	32.119680
617.775860	44545.823914	32.124698
618.759322	44628.800253	32.129716
619.259684	44721.508390	32.134733
619.610865	44801.101187	32.139751
620.064137	44887.206665	32.144768
620.808308	44973.242395	32.149786
621.777120	45059.396128	32.154804
622.441900	45152.079249	32.159821
623.404027	45229.009243	32.164839
624.367933	45305.812967	32.169856
624.798306	45400.383069	32.174874
625.758662	45463.210482	32.179892
626.148057	45541.436147	32.184909
626.627540	45617.793878	32.189927
627.433408	45697.801637	32.194944
627.611977	45783.470374	32.199962
628.480827	45851.779675	32.204980
629.132878	45936.420530	32.209997
629.626858	46019.963823	32.215015
630.549093	46098.492178	32.220032
630.960611	46178.917598	32.225050
631.746875	46252.003468	32.230068
632.325999	46333.020735	32.235085
632.869278	46404.956953	32.240103
633.405123	46476.954668	32.245120
633.743125	46561.681784	32.250138
635.016457	46623.605709	32.255156
635.319772	46705.664761	32.260173
636.092985	46759.976758	32.265191
636.725930	46831.833493	32.270208
636.645226	46911.576046	32.275226
637.276140	46980.749728	32.280244
637.551303	47065.928399	32.285261
638.297055	47163.947625	32.290279
638.963784	47244.824886	32.295296
639.342111	47344.838216	32.300314
640.033414	47440.679609	32.305332
640.830829	47537.283915	32.310349
641.434952	47635.070047	32.315367
642.248895	47723.295155	32.320384
642.927602	47806.222210	32.325402
643.725237	47885.868022	32.330420
644.306508	47989.318463	32.335437
644.955515	48078.516643	32.340455
645.729191	48161.979027	32.345472
646.133601	48260.925554	32.350490
646.941294	48340.085311	32.355508
647.640847	48440.452424	32.360525
647.988048	48533.387799	32.365543
649.032078	48617.107535	32.370560
649.428537	48716.907221	32.375578
650.249343	48802.003587	32.380596
651.264539	48887.488234	32.385613
651.459733	48986.444670	32.390631
652.244325	49069.429235	32.395648
652.828692	49158.314736	32.400666
653.692536	49258.763250	32.405684
654.624742	49349.783842	32.410701
655.332976	49421.521124	32.415719
656.150089	49510.979329	32.420736
656.768216	49605.735275	32.425754
657.211330	49679.870056	32.430772
657.780672	49770.096749	32.435789
658.259582	49861.409393	32.440807
659.257692	49945.802599	32.445824
659.645083	50041.293594	32.450842
660.694986	50136.249303	32.455860
661.285881	50219.937229	32.460877
661.768785	50307.458412	32.465895
662.656072	50399.044103	32.470912
663.153145	50500.169246	32.475930
664.027562	50574.599457	32.480948
664.555213	50665.907890	32.485965
664.816640	50765.898494	32.490983
665.424692	50851.958180	32.496000
666.092537	50952.624825	32.501018
666.893601	51033.663391	32.506036
667.871265	51115.816437	32.511053
668.802446	51217.328460	32.516071
669.325824	51295.922086	32.521088
669.644494	51392.138615	32.526106
670.407369	51494.722149	32.531124
670.976875	51586.858690	32.536141
671.327268	51691.220067	32.541159
672.188528	51773.167740	32.546176
672.624449	51882.771607	32.551194
673.157420	51973.753732	32.556212
674.046032	52082.007962	32.561229
674.672391	52181.860368	32.566247
675.720921	52276.011995	32.571264
675.973610	52370.541875	32.576282
676.884081	52475.645678	32.581300
677.455161	52558.551100	32.586317
678.039882	52642.408504	32.591335
679.026775	52735.347033	32.596352
679.148422	52831.151589	32.601370
679.928514	52917.169967	32.606388
680.587287	53017.750964	32.611405
681.190844	53128.013295	32.616423
682.033606	53204.925773	32.621440
682.573542	53299.659116	32.626458
682.974887	53402.451451	32.631476
684.401090	53493.103678	32.636493
684.103345	53599.986128	32.641511
685.607026	53707.620359	32.646528
686.117920	53802.980057	32.651546
686.308766	53895.638649	32.656564
687.567461	53999.928781	32.661581
688.090879	54102.584618	32.666599
688.913385	54200.958817	32.671616
689.609531	54304.067325	32.676634
690.013089	54405.297811	32.681652
690.764353	54513.780967	32.686669
691.315659	54628.331175	32.691687
692.266719	54713.716435	32.696704
692.811914	54822.159519	32.701722
693.422465	54931.672758	32.706740
694.400233	55040.190921	32.711757
695.076584	55140.982136	32.716775
695.986896	55260.436298	32.721792
696.547799	55370.244492	32.726810
697.420247	55464.927104	32.731828
698.042008	55571.257791	32.736845
698.745971	55679.243448	32.741863
699.407040	55772.951562	32.746880
700.368621	55883.151354	32.751898
701.215116	55982.756254	32.756916
701.989211	56081.078384	32.761933
702.528167	56195.507090	32.766951
703.555072	56274.189292	32.771968
704.152711	56369.060640	32.776986
704.681381	56478.747656	32.782004
705.396724	56575.464463	32.787021
705.805059	56688.426466	32.792039
706.852030	56784.786250	32.797056
707.286248	56892.172297	32.802074
707.867135	56998.195187	32.807092
708.803082	57110.320568	32.812109
709.296769	57222.266877	32.817127
710.322914	57325.071343	32.822144
710.594897	57426.187442	32.827162
711.339983	57540.027527	32.832180
712.337731	57647.760592	32.837197
712.652577	57749.446259	32.842215
713.580163	57858.588493	32.847232
714.164951	57987.730066	32.852250
714.830652	58101.592796	32.857268
715.991749	58197.630976	32.862285
716.561627	58313.020949	32.867303
717.152962	58415.283609	32.872320
717.676626	58523.820069	32.877338
718.663255	58643.819173	32.882356
719.577276	58753.069653	32.887373
720.040018	58862.787039	32.892391
720.702934	58969.697880	32.897408
721.227567	59078.066574	32.902426
722.313538	59190.298964	32.907444
723.246341	59301.400861	32.912461
723.960727	59407.553554	32.917479
724.525823	59509.093109	32.922496
725.519033	59616.306738	32.927514
726.260023	59704.914198	32.932532
727.343086	59782.362427	32.937549
727.831849	59875.277866	32.942567
728.751599	59959.275367	32.947584
729.502612	60057.387145	32.952602
729.705199	60155.425661	32.957620
730.646347	60244.981971	32.962637
731.381370	60348.273491	32.967655
731.962926	60453.429881	32.972672
732.599001	60548.390605	32.977690
733.059940	60647.128244	32.982708
733.837752	60749.681677	32.987725
734.103002	60871.645939	32.992743
735.182868	60979.332821	32.997760
735.985360	61097.531637	33.002778
736.338998	61219.660356	33.007796
737.511962	61315.427122	33.012813
738.065690	61429.466259	33.017831
738.410243	61542.459874	33.022848
739.080194	61651.974969	33.027866
739.684123	61782.553447	33.032884
741.014056	61898.438881	33.037901
741.302775	62012.581939	33.042919
742.077692	62136.087583	33.047936
742.993776	62253.484369	33.052954
743.411402	62373.846148	33.057972
744.611783	62499.603246	33.062989
745.146459	62637.744993	33.068007
745.821359	62758.553220	33.073024
746.650689	62875.266365	33.078042
747.358038	63000.425375	33.083060
748.473144	63110.291954	33.088077
748.969200	63244.013578	33.093095
750.005274	63369.992791	33.098112
750.758578	63483.542762	33.103130
752.274152	63590.008556	33.108148
753.479965	63690.660553	33.113165
754.320538	63807.705837	33.118183
754.829688	63904.637313	33.123200
755.994149	64012.541188	33.128218
756.428995	64124.175246	33.133236
757.696410	64213.246406	33.138253
757.912242	64320.606950	33.143271
758.395417	64416.540127	33.148288
759.241024	64524.878598	33.153306
759.643511	64651.431732	33.158324
760.592209	64744.091198	33.163341
761.153905	64868.463944	33.168359
761.500299	64983.246136	33.173376
762.850747	65095.815155	33.178394
763.240524	65211.362616	33.183412
764.192081	65334.649783	33.188429
765.153363	65450.742638	33.193447
765.418068	65568.828558	33.198464
766.266443	65686.332036	33.203482
766.884482	65811.409128	33.208500
767.947332	65920.079359	33.213517
768.459472	66045.080529	33.218535
769.276678	66164.975001	33.223552
769.833066	66287.188932	33.228570
770.591729	66405.589973	33.233588
771.540327	66533.594219	33.238605
772.410832	66660.082347	33.243623
772.862272	66778.378205	33.248640
773.670083	66903.892009	33.253658
774.261096	67029.429726	33.258676
775.516965	67140.546215	33.263693
775.999855	67260.717143	33.268711
776.534776	67378.003792	33.273728
777.641253	67481.725082	33.278746
778.489754	67602.349662	33.283764
779.404961	67719.973706	33.288781
780.031732	67832.228216	33.293799
780.591142	67936.149569	33.298816
781.876179	68056.028239	33.303834
782.249514	68182.791024	33.308852
783.224319	68281.935643	33.313869
783.907638	68401.795535	33.318887
784.646072	68534.133072	33.323904
785.478862	68639.846164	33.328922
786.002989	68777.227716	33.333940
786.930606	68896.790882	33.338957
787.651143	69019.094824	33.343975
787.972050	69154.331232	33.348992
789.055658	69279.048728	33.354010
789.639656	69407.781944	33.359028
790.104904	69538.413294	33.364045
791.272070	69666.988569	33.369063
791.822102	69806.496869	33.374080
792.413820	69939.575564	33.379098
793.111207	70083.215224	33.384116
794.202243	70222.535769	33.389133
794.955285	70358.941417	33.394151
795.503474	70502.867782	33.399168
796.460693	70639.367970	33.404186
797.397116	70782.226811	33.409204
798.667922	70925.809097	33.414221
799.291717	71055.361381	33.419239
800.097775	71206.830978	33.424256
800.833544	71335.803742	33.429274
801.693977	71480.380672	33.434292
802.731700	71611.151537	33.439309
804.011646	71749.287456	33.444327
804.825480	71871.548168	33.449344
805.585485	72013.995454	33.454362
806.112895	72138.347345	33.459380
806.640412	72270.072756	33.464397
808.154508	72408.945696	33.469415
808.931187	72540.581039	33.474432
809.866167	72655.617716	33.479450
810.291531	72802.071221	33.484468
811.355977	72935.394056	33.489485
811.934165	73056.404141	33.494503
812.501501	73201.072688	33.499520
813.695149	73338.031633	33.504538
814.307699	73475.586960	33.509556
814.870465	73602.673241	33.514573
815.700698	73746.657030	33.519591
816.329167	73892.161152	33.524608
817.751423	74029.295414	33.529626
817.769304	74162.039798	33.534644
818.580279	74306.220201	33.539661
819.993805	74444.433574	33.544679
820.463121	74596.627675	33.549696
821.598982	74726.838435	33.554714
822.197614	74871.911384	33.559732
823.237411	75002.323051	33.564749
824.158081	75143.505985	33.569767
824.911745	75287.063635	33.574784
826.134487	75411.186732	33.579802
827.082336	75552.570200	33.584820
827.695650	75685.851645	33.589837
828.714635	75813.874746	33.594855
829.325844	75950.516305	33.599872
830.330472	76084.121342	33.604890
830.870650	76210.587836	33.609908
831.662852	76335.078193	33.614925
832.652533	76467.151217	33.619943
833.184085	76593.558100	33.624960
834.026906	76723.038599	33.629978
834.207261	76854.785905	33.634996
835.238548	76980.827895	33.640013
836.055644	77129.908473	33.645031
836.523187	77265.721795	33.650048
837.512098	77396.927732	33.655066
838.263970	77537.135688	33.660084
838.713461	77692.858459	33.665101
840.389231	77846.374885	33.670119
840.815265	77990.763284	33.675136
841.942992	78127.522816	33.680154
842.819896	78279.656191	33.685172
843.390926	78424.693917	33.690189
844.375533	78574.433347	33.695207
844.986195	78728.359459	33.700224
846.526522	78867.667669	33.705242
847.466305	79010.814061	33.710260
848.206235	79166.632047	33.715277
848.976572	79311.250486	33.720295
850.061361	79445.994836	33.725312
850.859520	79589.111401	33.730330
851.558528	79724.882578	33.735348
852.132955	79881.820841	33.740365
853.501265	80027.705138	33.745383
854.348960	80169.697642	33.750400
855.185501	80330.922380	33.755418
856.022265	80473.140004	33.760436
856.708651	80615.250523	33.765453
857.776165	80770.563824	33.770471
858.534488	80912.544158	33.775488
859.307802	81054.099091	33.780506
860.160701	81201.164141	33.785524
860.898627	81357.794738	33.790541
861.652767	81508.142201	33.795559
862.401700	81666.544353	33.800576
863.456465	81818.634466	33.805594
864.561444	81975.853985	33.810612
865.086164	82133.480380	33.815629
865.626197	82286.746701	33.820647
866.671043	82459.592181	33.825664
867.774103	82615.108408	33.830682
868.896407	82761.038367	33.835700
869.505991	82929.189356	33.840717
870.535460	83075.914789	33.845735
871.262684	83239.626589	33.850752
872.417356	83390.825056	33.855770
873.230178	83540.372845	33.860788
873.946500	83699.541071	33.865805
874.782824	83854.375933	33.870823
875.373117	84028.067541	33.875840
876.428080	84174.068271	33.880858
877.343295	84339.022216	33.885876
878.056543	84513.703132	33.890893
879.561943	84653.375476	33.895911
880.067673	84808.359938	33.900928
881.004272	84972.694881	33.905946
881.879421	85130.416954	33.910964
882.550187	85283.960156	33.915981
883.658585	85444.398052	33.920999
884.755583	85615.626411	33.926016
885.410899	85771.997233	33.931034
886.108818	85932.607526	33.936052
886.956455	86090.214152	33.941069
888.172983	86243.363585	33.946087
888.671581	86407.679815	33.951104
889.601457	86551.501737	33.956122
890.481737	86707.702525	33.961140
891.406927	86858.322595	33.966157
892.454413	87009.012030	33.971175
893.142798	87175.864922	33.976192
893.882075	87322.216065	33.981210
894.848933	87476.199438	33.986228
895.666061	87635.934943	33.991245
897.085261	87783.011942	33.996263
898.452400	87928.972151	34.001280
899.209132	88080.267004	34.006298
900.332482	88224.896214	34.011316
900.610747	88380.043290	34.016333
901.923940	88529.857068	34.021351
902.747094	88693.351138	34.026368
903.604008	88837.933196	34.031386
904.661716	88991.949487	34.036404
904.899496	89151.765648	34.041421
905.967888	89296.986363	34.046439
907.262568	89468.267276	34.051456
908.119653	89619.125143	34.056474
908.988416	89765.527074	34.061492
909.787823	89939.164952	34.066509
910.937259	90085.687050	34.071527
911.451404	90259.051632	34.076544
912.259540	90411.789447	34.081562
913.118904	90595.161405	34.086580
913.530087	90770.590755	34.091597
914.556396	90942.224050	34.096615
915.508943	91111.364696	34.101632
916.433291	91289.402719	34.106650
917.594642	91459.087244	34.111668
918.287583	91630.774199	34.116685
919.469788	91802.963836	34.121703
920.539875	91988.115350	34.126720
921.580162	92149.951892	34.131738
922.700782	92309.643471	34.136756
923.434225	92494.417785	34.141773
924.557171	92654.294802	34.146791
925.505285	92826.163348	34.151808
926.255811	93002.559286	34.156826
927.397375	93168.341536	34.161844
928.345918	93333.574522	34.166861
929.021404	93503.404319	34.171879
930.047982	93679.848224	34.176896
930.754035	93851.010853	34.181914
931.751788	94026.240508	34.186932
932.398371	94213.023328	34.191949
933.603883	94378.702027	34.196967
934.223010	94563.473023	34.201984
935.410171	94754.974718	34.207002
936.354170	94923.725749	34.212020
937.157897	95105.894289	34.217037
938.328910	95285.009678	34.222055
939.177676	95466.318977	34.227072
939.779576	95646.195574	34.232090
940.977195	95824.728187	34.237108
941.458492	96009.229024	34.242125
942.303135	96197.215921	34.247143
943.478050	96379.946618	34.252160
944.292064	96565.599351	34.257178
945.341032	96750.955163	34.262196
946.225047	96934.181085	34.267213
947.311974	97128.610616	34.272231
948.420724	97323.512824	34.277248
949.566784	97495.501771	34.282266
950.957286	97657.165075	34.287284
951.512483	97831.450460	34.292301
952.596155	97989.969844	34.297319
953.550339	98164.476547	34.302336
954.246230	98349.535435	34.307354
955.501376	98507.738607	34.312372
956.187833	98677.671941	34.317389
956.767723	98848.503955	34.322407
957.661256	99031.775398	34.327424
958.763265	99202.042502	34.332442
960.071379	99374.213890	34.337460
960.430176	99552.253407	34.342477
961.673454	99740.549436	34.347495
962.565890	99918.712353	34.352512
963.100999	100109.071583	34.357530
964.711035	100291.866729	34.362548
965.236689	100474.025550	34.367565
966.254004	100657.522629	34.372583
967.291432	100850.020316	34.377600
967.900899	101035.550060	34.382618
968.962768	101234.187686	34.387636
969.890306	101434.235551	34.392653
970.436778	101630.846782	34.397671
971.884393	101822.986552	34.402688
972.430047	102038.657934	34.407706
973.793299	102228.383488	34.412724
974.672272	102436.127073	34.417741
975.738010	102638.928352	34.422759
976.543893	102842.565565	34.427776
977.283646	103045.335234	34.432794
978.594597	103254.210771	34.437812
979.191433	103468.182532	34.442829
980.201388	103676.383052	34.447847
981.305986	103888.634573	34.452864
982.450954	104094.764705	34.457882
983.915993	104289.326105	34.462900
984.625245	104507.726491	34.467917
985.593998	104715.359638	34.472935
986.766135	104925.139054	34.477952
987.638139	105138.034399	34.482970
988.354922	105349.867996	34.487988
989.788371	105559.413081	34.493005
990.565238	105766.788672	34.498023
991.399812	105976.828567	34.503040
992.416918	106191.335907	34.508058
994.424627	106375.375066	34.513076
995.572191	106582.543931	34.518093
997.037620	106774.628844	34.523111
998.076209	106973.574003	34.528128
998.737134	107171.126540	34.533146
1000.102370	107357.900289	34.538164
1000.853722	107557.492524	34.543181
1001.603462	107748.461491	34.548199
1002.858754	107938.031173	34.553216
1003.762036	108134.740302	34.558234
1004.757594	108331.726958	34.563252
1005.355399	108536.152133	34.568269
1006.637718	108730.231962	34.573287
1007.597693	108937.196889	34.578304
1008.420606	109129.759573	34.583322
1009.772802	109318.297137	34.588340
1010.734842	109531.953969	34.593357
1011.497938	109726.519393	34.598375
1012.507547	109919.791566	34.603392
1013.172199	110122.077203	34.608410
1014.025500	110331.312439	34.613428
1015.040563	110543.549902	34.618445
1015.908432	110749.986664	34.623463
1016.959868	110958.244043	34.628480
1018.154879	111154.863808	34.633498
1019.204557	111339.171384	34.638516
1020.103123	111552.816682	34.643533
1020.895043	111742.945721	34.648551
1022.168372	111941.470984	34.653568
1023.099099	112140.839625	34.658586
1024.126236	112331.592635	34.663604
1024.957286	112540.303858	34.668621
1026.216875	112734.504864	34.673639
1027.837938	112938.072327	34.678656
1027.918569	113146.063309	34.683674
1029.259921	113355.722576	34.688692
1030.317142	113557.132824	34.693709
1031.079307	113782.003844	34.698727
1032.213037	113980.174189	34.703744
1033.034940	114196.880424	34.708762
1033.989558	114405.420688	34.713780
1034.990360	114631.462702	34.718797
1035.577953	114856.548617	34.723815
1036.760590	115080.980695	34.728832
1037.888971	115305.702250	34.733850
1038.593509	115539.072411	34.738868
1039.864093	115773.934693	34.743885
1040.574859	116010.563683	34.748903
1041.436181	116235.514158	34.753920
1042.601416	116476.518931	34.758938
1043.706735	116708.730424	34.763956
1044.794253	116954.845218	34.768973
1046.346997	117193.308922	34.773991
1047.282081	117425.807807	34.779008
1047.814182	117660.909091	34.784026
1048.978986	117903.129731	34.789044
1050.108745	118142.368091	34.794061
1051.149491	118404.214036	34.799079
1052.377682	118653.563892	34.804096
1053.486674	118888.998189	34.809114
1054.539891	119120.351066	34.814132
1055.908876	119371.508480	34.819149
1057.676848	119599.541566	34.824167
1058.728480	119819.699454	34.829184
1059.812752	120066.500505	34.834202
1061.051639	120288.202245	34.839220
1062.375227	120516.100535	34.844237
1063.163027	120737.487380	34.849255
1064.581594	120969.187578	34.854272
1065.366070	121195.951091	34.859290
1066.685137	121408.448733	34.864308
1067.549813	121634.429459	34.869325
1068.538704	121885.392645	34.874343
1069.633253	122102.532222	34.879360
1070.609995	122337.813636	34.884378
1071.789359	122569.021124	34.889396
1072.733550	122795.694634	34.894413
1073.505655	123036.058901	34.899431
1074.695363	123270.894434	34.904448
1075.570710	123501.817273	34.909466
1076.685353	123747.351796	34.914484
1077.531261	123984.530790	34.919501
1078.578133	124222.806369	34.924519
1080.028161	124445.442452	34.929536
1081.042817	124694.030091	34.934554
1082.452558	124931.186906	34.939572
1083.332643	125158.940898	34.944589
1084.312210	125403.979090	34.949607
1085.604477	125637.764475	34.954624
1086.454629	125878.392249	34.959642
1087.415944	126120.777881	34.964660
1088.607276	126365.053873	34.969677
1089.380200	126592.519555	34.974695
1090.710611	126819.717483	34.979712
1091.617423	127037.240831	34.984730
1092.675225	127270.519896	34.989748
1093.979743	127500.388718	34.994765
1094.490811	127737.323019	34.999783
1095.959090	127975.900886	35.004800
1096.283951	128206.545104	35.009818
1097.560720	128452.661515	35.014836
1099.225967	128680.248944	35.019853
1100.364362	128938.737102	35.024871
1101.447014	129160.315068	35.029888
1102.465214	129409.637820	35.034906
1103.406126	129651.560493	35.039924
1104.565716	129896.693766	35.044941
1105.675187	130155.640485	35.049959
1106.707766	130405.222360	35.054976
1107.772120	130655.003792	35.059994
1108.798853	130910.979054	35.065012
1109.664201	131161.164965	35.070029
1110.680475	131415.105304	35.075047
1112.361341	131666.947890	35.080064
1113.239023	131928.026349	35.085082
1114.488775	132174.366773	35.090100
1116.070887	132422.314816	35.095117
1116.763649	132687.904723	35.100135
1117.906182	132932.075758	35.105152
1119.519287	133190.850224	35.110170
1120.908099	133438.863460	35.115188
1122.535356	133685.318073	35.120205
1122.965928	133938.335814	35.125223
1124.467509	134182.064158	35.130240
1125.225423	134442.067436	35.135258
1125.895920	134691.045604	35.140276
1127.080165	134952.022128	35.145293
1128.138170	135220.336326	35.150311
1129.423174	135470.638899	35.155328
1130.438220	135747.141386	35.160346
1131.513333	136009.969978	35.165364
1132.595446	136271.519097	35.170381
1133.634829	136540.252932	35.175399
1134.969209	136818.600753	35.180416
1136.055692	137086.900247	35.185434
1137.198859	137354.444570	35.190452
1138.523932	137630.886422	35.195469
1139.322471	137893.864496	35.200487
1140.959730	138170.373427	35.205504
1141.613611	138441.684019	35.210522
1142.752408	138703.876994	35.215540
1144.369725	138973.321281	35.220557
1144.766525	139263.825714	35.225575
1146.363816	139532.491730	35.230592
1147.694503	139800.722106	35.235610
1148.617622	140081.409314	35.240628
1150.220842	140355.292007	35.245645
1151.039608	140625.959090	35.250663
1152.396587	140898.187807	35.255680
1153.604194	141175.033321	35.260698
1154.774717	141429.621930	35.265716
1155.929079	141710.880388	35.270733
1156.933777	141991.886909	35.275751
1158.089930	142258.174789	35.280768
1159.233295	142529.234503	35.285786
1160.385333	142802.590007	35.290804
1161.367953	143069.394647	35.295821
1162.379926	143349.802400	35.300839
1163.819738	143633.387969	35.305856
1165.004012	143902.372111	35.310874
1166.324726	144173.859238	35.315892
1167.804096	144437.967513	35.320909
1168.932925	144686.601743	35.325927
1169.955329	144950.408890	35.330944
1171.119400	145202.616950	35.335962
1171.921820	145452.794146	35.340980
1173.375564	145715.660832	35.345997
1174.151639	145982.242792	35.351015
1175.582936	146236.024627	35.356032
1176.520711	146500.187018	35.361050
1177.580555	146787.512965	35.366068
1179.016795	147054.019340	35.371085
1180.037041	147329.968124	35.376103
1181.109540	147606.354264	35.381120
1182.365195	147877.132272	35.386138
1183.274945	148157.404791	35.391156
1184.570451	148438.275274	35.396173
1185.879027	148715.987917	35.401191
1186.728646	148997.202650	35.406208
1188.022675	149302.772426	35.411226
1189.055012	149580.587983	35.416244
1190.400729	149863.782055	35.421261
1191.079997	150169.321023	35.426279
1192.341392	150450.098456	35.431296
1193.855970	150747.793219	35.436314
1195.178564	151051.635255	35.441332
1196.691745	151326.670441	35.446349
1197.987687	151624.585888	35.451367
1198.994807	151915.423391	35.456384
1200.645338	152197.139085	35.461402
1201.655710	152501.716679	35.466420
1203.250730	152797.537364	35.471437
1204.257423	153075.586207	35.476455
1205.510801	153363.794109	35.481472
1207.375643	153644.495907	35.486490
1208.038006	153929.520538	35.491508
1209.527412	154215.565034	35.496525
1210.252510	154514.650270	35.501543
1211.786265	154798.928710	35.506560
1213.109397	155088.964645	35.511578
1214.262644	155375.885069	35.516596
1215.647684	155666.232232	35.521613
1216.682920	155951.869898	35.526631
1218.057979	156254.324220	35.531648
1219.179322	156537.668724	35.536666
1220.191503	156837.472913	35.541684
1221.143949	157132.151835	35.546701
1222.470307	157430.411864	35.551719
1223.684858	157726.003347	35.556736
1224.967593	158022.346900	35.561754
1225.905265	158328.656895	35.566772
1227.765762	158630.732208	35.571789
1228.713964	158934.013291	35.576807
1229.830127	159224.177352	35.581824
1231.453053	159528.061958	35.586842
1232.258749	159831.411398	35.591860
1233.707547	160130.648211	35.596877
1234.823930	160442.437845	35.601895
1235.821130	160735.194975	35.606912
1236.987957	161032.290270	35.611930
1238.237721	161349.494529	35.616948
1239.796264	161637.864810	35.621965
1240.644796	161950.154176	35.626983
1242.035023	162259.806489	35.632000
1243.212142	162572.566473	35.637018
1244.119386	162886.413674	35.642036
1245.308733	163195.421034	35.647053
1246.326351	163513.010045	35.652071
1247.662298	163818.331270	35.657088
1249.343799	164124.105163	35.662106
1250.304736	164422.476663	35.667124
1251.580470	164715.989806	35.672141
1252.684685	165025.354513	35.677159
1253.979238	165317.308145	35.682176
1255.530665	165617.011567	35.687194
1256.432352	165935.272240	35.692212
1258.065448	166229.726440	35.697229
1259.397815	166534.699784	35.702247
1260.393121	166834.148205	35.707264
1262.006056	167140.094539	35.712282
1263.092874	167452.080597	35.717300
1264.965895	167759.231785	35.722317
1266.007424	168050.509702	35.727335
1267.097969	168350.269999	35.732352
1268.606091	168659.390960	35.737370
1269.837416	168980.829626	35.742388
1271.146341	169282.197015	35.747405
1272.449073	169593.045965	35.752423
1273.397108	169910.058954	35.757440
1274.874946	170203.727919	35.762458
1276.153620	170531.755468	35.767476
1277.244366	170839.856439	35.772493
1278.324893	171159.838278	35.777511
1279.540977	171489.075863	35.782528
1280.870586	171806.343687	35.787546
1282.238893	172139.063091	35.792564
1283.303646	172459.297715	35.797581
1284.517274	172784.129018	35.802599
1285.671425	173126.877635	35.807616
1287.234702	173448.508818	35.812634
1288.447272	173795.935256	35.817652
1289.937729	174126.592963	35.822669
1291.412010	174448.106100	35.827687
1292.688607	174790.935495	35.832704
1294.243036	175111.906923	35.837722
1295.080303	175449.420207	35.842740
1297.013947	175783.645760	35.847757
1298.154966	176103.093074	35.852775
1299.310160	176444.685306	35.857792
1301.022394	176770.591123	35.862810
1302.058277	177110.164530	35.867828
1303.386588	177431.505994	35.872845
1304.604149	177759.860569	35.877863
1305.756789	178107.378857	35.882880
1307.291393	178439.683320	35.887898
1308.582095	178772.385620	35.892916
1309.874857	179118.225315	35.897933
1311.698473	179442.214035	35.902951
1313.234414	179771.024323	35.907968
1314.857469	180079.008217	35.912986
1316.085830	180404.624357	35.918004
1317.378006	180730.879330	35.923021
1318.932661	181061.014837	35.928039
1319.970059	181375.157224	35.933056
1321.107344	181687.660475	35.938074
1322.318276	182023.773345	35.943092
1323.743211	182357.352726	35.948109
1324.895566	182673.400533	35.953127
1326.080940	183002.022847	35.958144
1327.601632	183334.767664	35.963162
1328.664382	183673.111370	35.968180
1330.307383	183991.548452	35.973197
1331.596318	184328.069359	35.978215
1332.645616	184662.766113	35.983232
1333.954033	184990.466561	35.988250
1335.050108	185329.411816	35.993268
1336.607724	185648.774019	35.998285
1338.017349	185966.905917	36.003303
1338.893016	186291.030065	36.008320
1340.005230	186608.922841	36.013338
1340.876354	186948.435689	36.018356
1342.198819	187280.222082	36.023373
1343.484877	187617.258821	36.028391
1344.399167	187961.238795	36.033408
1345.995732	188315.745443	36.038426
1347.302014	188663.726945	36.043444
1348.400155	189016.581226	36.048461
1349.845659	189374.495949	36.053479
1350.825502	189728.859325	36.058496
1352.478739	190093.383126	36.063514
1353.460291	190449.692820	36.068532
1355.055131	190814.776638	36.073549
1356.659494	191178.807554	36.078567
1357.689448	191564.515718	36.083584
1359.199514	191932.959065	36.088602
1360.532621	192309.329815	36.093620
1361.967898	192684.670519	36.098637
1363.632683	193063.949089	36.103655
1364.344929	193433.028427	36.108672
1366.182100	193815.126853	36.113690
1367.316365	194200.606237	36.118708
1368.808072	194581.953998	36.123725
1370.363170	194958.393405	36.128743
1371.586665	195334.991380	36.133760
1373.282183	195717.023400	36.138778
1374.712841	196095.470634	36.143796
1375.850511	196491.830706	36.148813
1377.688909	196870.697699	36.153831
1378.746751	197258.569842	36.158848
1380.492369	197638.053363	36.163866
1381.887893	198019.628175	36.168884
1382.911255	198406.674978	36.173901
1384.970612	198793.032572	36.178919
1386.169514	199163.994801	36.183936
1387.506439	199542.236438	36.188954
1388.961136	199933.436013	36.193972
1390.433248	200323.809752	36.198989
1391.838474	200694.987634	36.204007
1393.294957	201084.517694	36.209024
1394.711597	201468.851100	36.214042
1395.866204	201857.838641	36.219060
1397.485516	202242.307949	36.224077
1398.973573	202616.186829	36.229095
1400.417944	203010.998718	36.234112
1402.222701	203394.123288	36.239130
1403.639818	203777.275800	36.244148
1404.886161	204165.461038	36.249165
1406.310208	204535.945146	36.254183
1407.278435	204920.244328	36.259200
1408.660500	205300.604681	36.264218
1410.097383	205699.000327	36.269236
1411.612176	206085.475442	36.274253
1413.720606	206463.347540	36.279271
1415.019391	206853.772964	36.284288
1416.642054	207232.186170	36.289306
1417.966151	207612.478930	36.294324
1418.879826	207990.479594	36.299341
1421.071225	208366.874531	36.304359
1422.272484	208749.415188	36.309376
1423.797283	209141.833782	36.314394
1425.145830	209499.288850	36.319412
1426.439879	209880.511807	36.324429
1427.886807	210272.910721	36.329447
1429.282676	210648.812864	36.334464
1430.784535	210994.034005	36.339482
1431.722803	211363.919992	36.344500
1433.245711	211723.730576	36.349517
1434.467556	212079.859187	36.354535
1435.879987	212465.087164	36.359552
1437.324928	212832.254831	36.364570
1438.701805	213213.631846	36.369588
1439.821980	213590.913296	36.374605
1441.240495	213971.093153	36.379623
1442.049205	214362.752991	36.384640
1443.818262	214758.649729	36.389658
1444.935397	215160.801854	36.394676
1446.019464	215557.958032	36.399693
1447.641107	215961.097148	36.404711
1448.804162	216368.351876	36.409728
1450.182536	216785.020676	36.414746
1451.664558	217198.169391	36.419764
1453.000000	217613.655290	36.424781
1454.439265	218028.211560	36.429799
1455.946575	218444.637830	36.434816
1457.426774	218921.822111	36.439834
1459.374304	219376.936921	36.444852
1460.334845	219806.589990	36.449869
1461.888030	220226.495783	36.454887
1463.486132	220663.869964	36.459904
1464.799654	221094.689384	36.464922
1466.422125	221527.161324	36.469940
1467.696012	221970.182224	36.474957
1469.226287	222405.720838	36.479975
1470.742537	222848.756209	36.484992
1472.225764	223281.359871	36.490010
1473.923362	223715.479216	36.495028
1475.995851	224160.180654	36.500045
1478.104526	224574.322575	36.505063
1479.295685	225009.698882	36.510080
1480.645930	225427.093180	36.515098
1482.444787	225863.515410	36.520116
1483.983398	226299.499615	36.525133
1485.775169	226717.028842	36.530151
1487.776856	227144.532407	36.535168
1489.156134	227551.490058	36.540186
1491.155973	227950.675855	36.545204
1492.690279	228374.806415	36.550221
1494.291179	228771.825447	36.555239
1495.583345	229183.831990	36.560256
1497.021709	229605.899639	36.565274
1498.621855	230010.720483	36.570292
1499.770684	230434.489577	36.575309
1501.129538	230840.089354	36.580327
1502.520437	231255.692889	36.585344
1503.676330	231676.924600	36.590362
1505.769393	232097.113900	36.595380
1507.003216	232521.611958	36.600397
1508.715928	232942.196697	36.605415
1509.936886	233372.185947	36.610432
1511.454179	233785.362831	36.615450
1512.934326	234206.370517	36.620468
1514.324383	234644.692437	36.625485
1515.725511	235061.575079	36.630503
1517.390091	235497.161528	36.635520
1518.797297	235927.101699	36.640538
1520.000290	236363.350851	36.645556
1521.380642	236793.272288	36.650573
1523.056673	237235.846817	36.655591
1524.353322	237682.498535	36.660608
1525.640969	238116.045568	36.665626
1527.257207	238568.438350	36.670644
1528.641653	239006.594647	36.675661
1529.961520	239437.980308	36.680679
1531.388587	239872.727709	36.685696
1533.298773	240294.212706	36.690714
1534.962381	240722.242208	36.695732
1536.131612	241156.145864	36.700749
1537.650482	241586.436422	36.705767
1539.435008	242031.620521	36.710784
1540.279295	242465.605850	36.715802
1542.005121	242898.303455	36.720820
1543.317313	243348.673973	36.725837
1544.992280	243792.584080	36.730855
1546.299719	244256.776012	36.735872
1547.715289	244705.353822	36.740890
1549.420547	245153.732203	36.745908
1551.068100	245622.188928	36.750925
1552.824957	246071.322413	36.755943
1554.280665	246525.790069	36.760960
1555.386313	246994.262298	36.765978
1557.592626	247455.034431	36.770996
1558.904779	247929.316664	36.776013
1560.777189	248396.318151	36.781031
1562.593492	248863.532775	36.786048
1563.983096	249326.982596	36.791066
1565.337595	249794.909724	36.796084
1567.412424	250264.318968	36.801101
1568.891011	250723.716758	36.806119
1570.522737	251193.708261	36.811136
1571.949228	251664.521635	36.816154
1573.656793	252143.621331	36.821172
1575.245895	252611.208043	36.826189
1576.882255	253077.390217	36.831207
1578.386230	253561.808697	36.836224
1579.799439	254040.222011	36.841242
1581.489859	254522.502048	36.846260
1582.812592	255002.734637	36.851277
1584.511660	255485.242548	36.856295
1586.109060	255964.439705	36.861312
1587.834707	256463.024052	36.866330
1589.568656	256942.148384	36.871348
1590.767209	257437.314522	36.876365
1592.402050	257930.681445	36.881383
1593.783843	258420.533822	36.886400
1595.339123	258920.315800	36.891418
1597.259783	259423.797288	36.896436
1598.595644	259928.569298	36.901453
1600.036930	260422.959410	36.906471
1601.651388	260928.041161	36.911488
1603.178952	261437.608215	36.916506
1605.198230	261948.999338	36.921524
1606.677097	262455.246465	36.926541
1608.463464	262956.666926	36.931559
1609.900568	263457.586000	36.936576
1611.787928	263966.178613	36.941594
1612.922020	264470.144891	36.946612
1614.660386	264985.950761	36.951629
1616.187281	265505.601726	36.956647
1617.776899	266005.097270	36.961664
1619.525452	266520.468670	36.966682
1622.069328	267016.224227	36.971700
1623.467062	267529.798301	36.976717
1625.063786	268036.937510	36.981735
1627.013415	268543.586177	36.986752
1628.623715	269031.390436	36.991770
1630.187177	269542.775980	36.996788
1631.737815	270046.694580	37.001805
1632.917665	270544.323022	37.006823
1635.020215	271055.897281	37.011840
1635.947321	271555.141161	37.016858
1637.437492	272048.880659	37.021876
1638.392057	272556.679426	37.026893
1640.212642	273051.683949	37.031911
1641.930686	273556.941974	37.036928
1643.403484	274065.694431	37.041946
1645.055508	274566.617838	37.046964
1646.582098	275080.287822	37.051981
1647.891192	275597.422112	37.056999
1649.742384	276102.831611	37.062016
1651.260715	276638.447852	37.067034
1652.609847	277161.643680	37.072052
1654.163547	277692.044340	37.077069
1655.598949	278226.095881	37.082087
1657.625483	278767.415334	37.087104
1659.052063	279306.393859	37.092122
1660.597076	279838.518337	37.097140
1662.058738	280391.332549	37.102157
1664.138536	280935.050984	37.107175
1666.324689	281475.397347	37.112192
1667.721382	282016.685332	37.117210
1670.046235	282561.019285	37.122228
1671.732680	283105.253764	37.127245
1673.614236	283637.795060	37.132263
1675.163453	284177.095613	37.137280
1676.972798	284736.850595	37.142298
1679.081159	285271.915017	37.147316
1680.741669	285815.738862	37.152333
1682.490409	286353.577034	37.157351
1684.532159	286887.681878	37.162368
1685.973834	287435.346466	37.167386
1687.840326	287971.381552	37.172404
1689.552723	288515.416024	37.177421
1690.845413	289052.405496	37.182439
1692.861177	289592.677369	37.187456
1694.087506	290162.110311	37.192474
1695.918945	290695.245364	37.197492
1697.452957	291260.584310	37.202509
1698.895422	291813.591423	37.207527
1700.685446	292365.014854	37.212544
1702.088006	292932.908299	37.217562
1703.755399	293504.667100	37.222580
1705.567596	294070.938418	37.227597
1707.520539	294630.097372	37.232615
1709.757274	295199.773143	37.237632
1711.439094	295767.073970	37.242650
1713.000507	296317.907712	37.247668
1714.734186	296882.222781	37.252685
1716.499034	297450.771536	37.257703
1718.528961	298017.825907	37.262720
1720.152471	298587.611266	37.267738
1721.710588	299150.013376	37.272756
1723.062942	299729.260306	37.277773
1724.955575	300303.386008	37.282791
1726.595849	300864.546221	37.287808
1727.807616	301450.537220	37.292826
1729.722948	302035.519791	37.297844
1731.285930	302606.435826	37.302861
1732.643797	303208.773898	37.307879
1734.973695	303786.997963	37.312896
1736.332702	304372.921690	37.317914
1738.725631	304951.509161	37.322932
1740.685303	305533.364507	37.327949
1742.237895	306111.727725	37.332967
1744.275581	306699.810332	37.337984
1745.733486	307279.502239	37.343002
1747.765071	307844.746709	37.348020
1749.360882	308434.592130	37.353037
1750.595335	309022.689977	37.358055
1752.885036	309584.705859	37.363072
1754.174439	310146.882976	37.368090
1755.861146	310699.467398	37.373108
1757.651135	311271.839418	37.378125
1759.446546	311835.953054	37.383143
1761.031626	312388.593467	37.388160
1762.926708	312972.566862	37.393178
1764.450241	313540.725545	37.398196
1766.402856	314112.466062	37.403213
1767.926669	314690.545418	37.408231
1769.670197	315273.383581	37.413248
1771.117241	315862.055909	37.418266
1773.269380	316433.644283	37.423284
1775.074369	317030.348789	37.428301
1776.391010	317624.030968	37.433319
1778.167375	318219.866979	37.438336
1779.964699	318822.245870	37.443354
1781.926883	319421.215185	37.448372
1783.493299	320015.191544	37.453389
1785.183245	320632.655518	37.458407
1787.526730	321243.480363	37.463424
1788.787624	321850.110891	37.468442
1790.486968	322463.163787	37.473460
1792.280708	323082.492441	37.478477
1793.625935	323713.315152	37.483495
1795.829003	324333.706968	37.488512
1797.420896	324961.531447	37.493530
1799.282117	325592.479066	37.498548
1800.913009	326229.831227	37.503565
1802.681185	326868.931496	37.508583
1805.051642	327501.349926	37.513600
1807.065770	328150.882103	37.518618
1808.943068	328774.101600	37.523636
1811.188920	329404.667297	37.528653
1812.717534	330059.717428	37.533671
1815.035518	330678.883652	37.538688
1816.572547	331323.153719	37.543706
1818.382548	331962.294069	37.548724
1820.298061	332586.101378	37.553741
1821.413244	333233.745261	37.558759
1823.670577	333878.705389	37.563776
1825.650806	334532.385897	37.568794
1827.706712	335168.885214	37.573812
1829.446196	335815.583634	37.578829
1830.819033	336463.502564	37.583847
1832.818732	337117.377343	37.588864
1834.208603	337767.257748	37.593882
1836.333988	338435.387236	37.598900
1838.373376	339071.208321	37.603917
1840.357157	339733.734656	37.608935
1842.514917	340387.491843	37.613952
1844.235637	341028.011955	37.618970
1845.966242	341679.970050	37.623988
1847.643986	342328.324097	37.629005
1849.030914	342994.307598	37.634023
1851.268204	343658.238238	37.639040
1853.019888	344319.676473	37.644058
1854.901473	344989.003246	37.649076
1856.923346	345651.013311	37.654093
1858.419124	346316.578155	37.659111
1860.203173	346985.893170	37.664128
1862.248859	347651.526236	37.669146
1864.199577	348316.201099	37.674164
1866.191285	348986.950681	37.679181
1867.910351	349661.872219	37.684199
1869.905737	350321.815786	37.689216
1871.861074	350985.766099	37.694234
1873.811408	351652.422874	37.699252
1875.998009	352279.163167	37.704269
1877.792374	352922.505041	37.709287
1879.576559	353554.927343	37.714304
1881.756898	354184.001667	37.719322
1883.331130	354828.849103	37.724340
1885.091855	355459.496717	37.729357
1886.850720	356117.895633	37.734375
1888.745053	356755.860877	37.739392
1890.088713	357407.178076	37.744410
1891.913866	358064.140272	37.749428
1893.783420	358714.310128	37.754445
1895.760149	359377.164020	37.759463
1897.515785	360047.630149	37.764480
1899.295578	360718.614149	37.769498
1901.101523	361389.151464	37.774516
1903.418170	362068.321171	37.779533
1904.795882	362748.116318	37.784551
1906.769250	363434.448706	37.789568
1908.771404	364122.083709	37.794586
1910.479573	364807.294346	37.799604
1912.867890	365493.902948	37.804621
1914.595712	366201.156998	37.809639
1916.578485	366885.017277	37.814656
1918.592539	367590.777956	37.819674
1920.552062	368285.829558	37.824692
1922.786586	368974.912567	37.829709
1924.623351	369673.332646	37.834727
1926.756253	370365.805940	37.839744
1928.891073	371054.461191	37.844762
1930.601391	371751.214292	37.849780
1932.410098	372450.677286	37.854797
1934.306688	373166.269198	37.859815
1936.248935	373877.705193	37.864832
1938.640504	374587.480504	37.869850
1940.493125	375296.544376	37.874868
1942.401849	375984.255445	37.879885
1944.478594	376707.304624	37.884903
1946.534887	377413.122214	37.889920
1948.422682	378123.644986	37.894938
1950.218766	378844.413711	37.899956
1952.328653	379550.787567	37.904973
1954.091393	380263.315585	37.909991
1956.194456	380998.696446	37.915008
1958.289933	381710.910961	37.920026
1960.177760	382430.625013	37.925044
1962.257213	383143.242815	37.930061
1964.030597	383879.020578	37.935079
1966.013197	384597.607106	37.940096
1968.118811	385321.761070	37.945114
1970.036636	386052.851696	37.950132
1971.987474	386766.907979	37.955149
1973.890931	387499.514876	37.960167
1975.841516	388222.767477	37.965184
1977.656713	388950.969671	37.970202
1979.729065	389693.284237	37.975220
1982.144020	390401.732017	37.980237
1983.703418	391143.006867	37.985255
1985.763218	391873.813513	37.990272
1988.226826	392605.854485	37.995290
1989.769333	393342.161801	38.000308
1992.011601	394075.877272	38.005325
1993.762415	394812.773858	38.010343
1995.685403	395562.981848	38.015360
1997.344527	396307.182322	38.020378
1999.491595	397040.968251	38.025396
2001.762264	397779.480560	38.030413
2003.645159	398521.586613	38.035431
2005.607651	399249.569850	38.040448
2007.279804	399968.510137	38.045466
2009.376872	400688.756458	38.050484
2011.622538	401397.024468	38.055501
2013.541853	402114.223641	38.060519
2015.716154	402820.415794	38.065536
2017.660427	403537.853969	38.070554
2019.771921	404257.020209	38.075572
2022.325976	404957.446034	38.080589
2024.320470	405695.218733	38.085607
2025.878050	406419.919393	38.090624
2027.985710	407125.558752	38.095642
2030.097917	407859.656961	38.100660
2031.928382	408583.090646	38.105677
2033.964338	409317.162563	38.110695
2035.529426	410057.499210	38.115712
2037.445884	410793.248448	38.120730
2039.472955	411541.245682	38.125748
2041.649830	412290.261356	38.130765
2043.808838	413043.463981	38.135783
2045.703262	413804.718664	38.140800
2047.799453	414557.002197	38.145818
2049.879499	415313.446204	38.150836
2051.872776	416081.052431	38.155853
2053.856725	416846.282192	38.160871
2055.984707	417605.539233	38.165888
2058.391429	418378.581277	38.170906
2060.435381	419151.128096	38.175924
2062.424607	419917.380191	38.180941
2064.204804	420709.321837	38.185959
2066.041293	421478.059107	38.190976
2068.548182	422261.526426	38.195994
2069.884712	423058.683836	38.201012
2072.886761	423833.917509	38.206029
2075.313885	424603.119781	38.211047
2077.410389	425393.747082	38.216064
2079.689629	426171.507939	38.221082
2081.873522	426958.627204	38.226100
2083.818822	427742.114849	38.231117
2085.597737	428525.098330	38.236135
2087.467155	429326.774424	38.241152
2089.377545	430118.696490	38.246170
2091.544130	430919.055283	38.251188
2093.131911	431725.658801	38.256205
2095.289391	432527.635500	38.261223
2097.157164	433357.980419	38.266240
2099.467697	434181.085651	38.271258
2101.362574	435000.282269	38.276276
2103.313504	435821.060472	38.281293
2105.465711	436652.152176	38.286311
2107.519852	437487.886342	38.291328
2110.163204	438304.159819	38.296346
2112.023983	439135.361339	38.301364
2114.538571	439964.805198	38.306381
2116.686010	440790.331991	38.311399
2118.318343	441616.925471	38.316416
2120.848059	442455.079817	38.321434
2122.613401	443299.248735	38.326452
2124.912777	444123.261065	38.331469
2126.563305	444971.685830	38.336487
2128.259955	445818.400653	38.341504
2130.935983	446668.917876	38.346522
2133.390596	447520.956033	38.351540
2135.241187	448365.168689	38.356557
2138.069644	449215.712513	38.361575
2139.647358	450057.475664	38.366592
2142.073155	450896.536742	38.371610
2143.893998	451754.429323	38.376628
2146.073851	452587.091137	38.381645
2148.024582	453413.739399	38.386663
2150.327991	454234.228164	38.391680
2152.127582	455057.751481	38.396698
2154.334886	455885.827325	38.401716
2156.599037	456703.494430	38.406733
2158.422473	457529.191074	38.411751
2160.488115	458350.263906	38.416768
2162.638571	459194.699522	38.421786
2164.379457	460044.729126	38.426804
2166.542793	460884.390408	38.431821
2168.534075	461739.767619	38.436839
2170.297613	462599.190173	38.441856
2172.892247	463471.733483	38.446874
2174.797693	464336.466724	38.451892
2176.500282	465219.341660	38.456909
2178.961404	466099.777586	38.461927
2181.158914	466986.939534	38.466944
2183.997043	467862.887600	38.471962
2185.934765	468743.189841	38.476980
2188.321912	469628.380942	38.481997
2190.777991	470517.057357	38.487015
2192.871706	471406.005113	38.492032
2195.416747	472296.757226	38.497050
2197.700940	473188.470713	38.502068
2199.829939	474079.207982	38.507085
2202.105279	474972.253604	38.512103
2204.186448	475878.979202	38.517120
2206.435042	476773.863255	38.522138
2208.304563	477673.565636	38.527156
2210.432958	478587.021644	38.532173
2212.668251	479492.535695	38.537191
2214.349540	480417.692712	38.542208
2216.983856	481331.232283	38.547226
2219.524152	482263.578297	38.552244
2221.742400	483175.932509	38.557261
2225.015692	484098.569800	38.562279
2226.753412	485023.988203	38.567296
2229.229251	485946.662227	38.572314
2231.541695	486858.662741	38.577332
2233.690317	487776.398833	38.582349
2236.045027	488699.303603	38.587367
2237.751756	489640.237701	38.592384
2240.321932	490561.696944	38.597402
2242.366919	491486.424647	38.602420
2244.535988	492429.454482	38.607437
2246.462357	493351.629548	38.612455
2248.806212	494291.854390	38.617472
2251.471978	495231.823442	38.622490
2253.919564	496161.836238	38.627508
2256.715270	497080.539376	38.632525
2259.412626	498009.703770	38.637543
2261.548720	498928.667945	38.642560
2263.713620	499852.016900	38.647578
2266.080293	500778.560914	38.652596
2267.969427	501712.799877	38.657613
2270.388204	502635.600374	38.662631
2272.504687	503556.835863	38.667648
2274.897823	504491.440728	38.672666
2277.302068	505421.098798	38.677684
2279.286884	506348.504037	38.682701
2281.903024	507282.308088	38.687719
2283.959145	508219.428496	38.692736
2286.337701	509146.861612	38.697754
2288.633897	510077.633106	38.702772
2290.686471	511006.878499	38.707789
2292.808626	511936.260230	38.712807
2294.818401	512893.734856	38.717824
2297.434476	513813.095934	38.722842
2299.524162	514735.867513	38.727860
2300.987910	515657.982779	38.732877
2303.647827	516582.971443	38.737895
2305.571430	517499.762208	38.742912
2307.353754	518423.678065	38.747930
2309.795426	519367.535401	38.752948
2311.584891	520313.911684	38.757965
2314.556233	521243.207386	38.762983
2316.415007	522202.505326	38.768000
2318.636375	523146.066836	38.773018
2320.936192	524109.857435	38.778036
2323.385180	525083.837807	38.783053
2325.626711	526056.933543	38.788071
2327.567774	527030.217541	38.793088
2330.478737	527995.573554	38.798106
2332.364471	528969.294893	38.803124
2334.710664	529964.226646	38.808141
2337.079573	530954.757967	38.813159
2338.949134	531958.496187	38.818176
2341.212666	532952.133216	38.823194
2343.782440	533959.193979	38.828212
2345.811532	534974.076733	38.833229
2348.409448	536001.780932	38.838247
2350.854121	537025.411354	38.843264
2353.147997	538043.357759	38.848282
2355.477746	539083.267415	38.853300
2357.763951	540118.479652	38.858317
2360.363952	541149.087223	38.863335
2362.704995	542204.969387	38.868352
2365.117155	543241.242054	38.873370
2367.334358	544278.326071	38.878388
2370.140534	545324.391201	38.883405
2372.152776	546378.154229	38.888423
2374.492366	547433.041152	38.893440
2377.261679	548483.402203	38.898458
2379.940440	549530.681544	38.903476
2382.203362	550593.486828	38.908493
2385.016035	551649.985623	38.913511
2387.067442	552714.924102	38.918528
2389.436588	553771.633844	38.923546
2392.202507	554829.603533	38.928564
2394.585380	555895.143241	38.933581
2396.692897	556962.453529	38.938599
2399.104337	558025.659031	38.943616
2401.406077	559099.049126	38.948634
2403.724519	560175.867341	38.953652
2406.257416	561248.141804	38.958669
2408.566177	562319.210995	38.963687
2411.041532	563407.898062	38.968704
2413.421616	564480.688640	38.973722
2415.887539	565559.856217	38.978740
2417.939246	566666.021482	38.983757
2420.951606	567754.710140	38.988775
2423.550713	568827.809698	38.993792
2425.934899	569914.210756	38.998810
2428.727080	571000.402570	39.003828
2431.022129	572073.984215	39.008845
2433.748895	573155.485815	39.013863
2436.225698	574236.635510	39.018880
2438.773566	575317.580877	39.023898
2441.130249	576393.647726	39.028916
2443.268295	577491.837218	39.033933
2445.772433	578563.629405	39.038951
2448.244701	579648.479209	39.043968
2450.566102	580734.563601	39.048986
2453.182330	581821.106193	39.054004
2455.162438	582905.752172	39.059021
2457.646556	583976.678585	39.064039
2460.174785	585054.073531	39.069056
2462.746622	586109.704625	39.074074
2465.184084	587158.898802	39.079092
2466.886994	588225.971178	39.084109
2469.724790	589291.007836	39.089127
2471.573121	590359.973174	39.094144
2473.917593	591424.300888	39.099162
2476.406014	592504.547508	39.104180
2478.847387	593597.833373	39.109197
2481.072152	594680.281403	39.114215
2483.478519	595786.900350	39.119232
2485.427319	596886.928223	39.124250
2488.134407	597998.049315	39.129268
2490.293039	599132.045861	39.134285
2492.663659	600250.672078	39.139303
2495.111252	601380.596052	39.144320
2497.488756	602533.505471	39.149338
2499.930886	603670.567733	39.154356
2502.207133	604816.306247	39.159373
2504.887680	605971.475013	39.164391
2507.288022	607148.596825	39.169408
2509.387692	608321.943051	39.174426
2512.126852	609503.619995	39.179444
2514.383811	610693.709389	39.184461
2516.999227	611870.205350	39.189479
2519.773029	613074.217029	39.194496
2522.332854	614268.680319	39.199514
2525.080816	615460.983986	39.204532
2527.412237	616665.881156	39.209549
2530.474554	617867.326349	39.214567
2533.042453	619076.822178	39.219584
2535.208384	620282.301584	39.224602
2537.846534	621488.770195	39.229620
2540.441247	622707.008639	39.234637
2543.009873	623930.662414	39.239655
2545.987727	625161.656303	39.244672
2548.473346	626384.996004	39.249690
2551.033838	627591.747077	39.254708
2553.606909	628827.833737	39.259725
2556.362851	630051.809249	39.264743
2558.799181	631285.335735	39.269760
2561.044254	632500.722659	39.274778
2563.739126	633740.012780	39.279796
2566.226282	634983.834335	39.284813
2569.100133	636208.924238	39.289831
2571.805351	637456.010345	39.294848
2574.246672	638707.781779	39.299866
2577.144387	639942.410092	39.304884
2579.558406	641187.249322	39.309901
2582.134999	642430.664081	39.314919
2584.768529	643684.045331	39.319936
2587.590285	644930.558312	39.324954
2590.343283	646167.205138	39.329972
2592.779309	647422.752542	39.334989
2595.221103	648668.021739	39.340007
2598.062131	649920.748826	39.345024
2600.494841	651175.580342	39.350042
2603.498959	652411.171021	39.355060
2605.414014	653674.097730	39.360077
2608.502058	654923.316724	39.365095
2611.218612	656174.432370	39.370112
2613.750189	657427.313030	39.375130
2616.453076	658681.002174	39.380148
2618.467939	659933.997047	39.385165
2621.638593	661186.690629	39.390183
2624.627000	662435.070756	39.395200
2626.953162	663681.607281	39.400218
2630.058361	664915.908201	39.405236
2632.307048	666126.899327	39.410253
2635.069331	667339.594075	39.415271
2637.803862	668560.698386	39.420288
2639.965075	669767.412347	39.425306
2643.020272	670963.478785	39.430324
2645.528779	672197.087792	39.435341
2648.194065	673410.915134	39.440359
2650.520287	674619.022899	39.445376
2653.031091	675845.838671	39.450394
2655.788427	677068.724547	39.455412
2658.392844	678306.685853	39.460429
2660.896494	679530.980448	39.465447
2663.394119	680765.947731	39.470464
2666.075228	682014.185075	39.475482
2668.396586	683272.248721	39.480500
2670.884586	684539.252532	39.485517
2673.799835	685798.510838	39.490535
2676.151900	687065.782710	39.495552
2678.477285	688341.273727	39.500570
2681.253766	689636.021753	39.505588
2684.086530	690917.470248	39.510605
2686.644771	692211.785086	39.515623
2689.306590	693515.721796	39.520640
2691.544495	694828.618187	39.525658
2694.435727	696137.393550	39.530676
2697.000883	697464.432338	39.535693
2699.542023	698798.417836	39.540711
2702.709576	700119.156052	39.545728
2705.102239	701454.053047	39.550746
2707.837491	702800.091899	39.555764
2710.345665	704152.602385	39.560781
2713.563691	705499.383996	39.565799
2716.263680	706830.681553	39.570816
2718.909228	708191.012653	39.575834
2721.808764	709541.972897	39.580852
2725.048760	710905.442167	39.585869
2727.348366	712261.173856	39.590887
2730.226426	713611.891248	39.595904
2732.684535	714987.313344	39.600922
2736.215901	716346.200142	39.605940
2738.959338	717700.296839	39.610957
2741.831331	719060.487665	39.615975
2744.808980	720427.069470	39.620992
2747.101945	721788.149296	39.626010
2750.229726	723154.061854	39.631028
2753.061740	724524.940793	39.636045
2755.275254	725901.973132	39.641063
2758.219293	727273.267386	39.646080
2760.858329	728639.786962	39.651098
2763.710418	730025.462742	39.656116
2766.473789	731411.906075	39.661133
2768.931857	732798.212918	39.666151
2772.021969	734179.733795	39.671168
2774.688251	735568.297750	39.676186
2777.249456	736956.096652	39.681204
2779.919032	738361.457522	39.686221
2782.778504	739762.986909	39.691239
2785.482791	741151.515385	39.696256
2788.777436	742545.772400	39.701274
2791.574015	743934.637470	39.706292
2794.813031	745330.632511	39.711309
2797.495393	746723.266582	39.716327
2800.574459	748107.749248	39.721344
2803.035382	749516.882704	39.726362
2805.901544	750907.213427	39.731380
2808.430274	752302.130608	39.736397
2811.294139	753697.775915	39.741415
2814.056074	755081.364073	39.746432
2816.532999	756451.945948	39.751450
2819.459418	757796.161279	39.756468
2821.819725	759162.879672	39.761485
2824.215822	760532.940317	39.766503
2827.067978	761895.788991	39.771520
2829.389333	763284.754804	39.776538
2832.135852	764676.149970	39.781556
2835.121023	766074.232938	39.786573
2837.706196	767448.172321	39.791591
2840.361029	768860.395061	39.796608
2842.637948	770286.275083	39.801626
2846.132155	771700.769967	39.806644
2848.641456	773126.065848	39.811661
2851.081381	774571.781515	39.816679
2853.891838	776017.692436	39.821696
2856.630335	777458.713841	39.826714
2859.008312	778928.725281	39.831732
2861.746132	780397.448189	39.836749
2864.785815	781881.775434	39.841767
2867.644047	783365.484714	39.846784
2870.195388	784859.438284	39.851802
2872.945168	786355.305081	39.856820
2875.825730	787860.253695	39.861837
2878.504927	789391.639207	39.866855
2881.766154	790910.589896	39.871872
2884.349408	792447.361970	39.876890
2887.026082	793985.009600	39.881908
2889.933553	795521.401942	39.886925
2892.757541	797082.694362	39.891943
2896.228227	798625.464001	39.896960
2899.020697	800188.124139	39.901978
2902.387594	801742.850128	39.906996
2905.868784	803293.538472	39.912013
2908.567201	804849.584462	39.917031
2911.447168	806403.487943	39.922048
2914.393870	807972.578072	39.927066
2917.350444	809542.919631	39.932084
2920.256970	811104.060868	39.937101
2923.543426	812671.279503	39.942119
2926.065675	814237.186236	39.947136
2928.965129	815812.972852	39.952154
2932.029169	817400.668118	39.957172
2934.974199	818977.852296	39.962189
2937.723162	820571.876257	39.967207
2940.761698	822157.956049	39.972224
2943.678565	823754.603998	39.977242
2946.410671	825352.408494	39.982260
2949.628805	826960.277384	39.987277
2952.505001	828557.474061	39.992295
2955.634989	830147.025915	39.997312
2958.333749	831752.583819	40.002330
2961.264793	833362.285599	40.007348
2964.249506	834982.146215	40.012365
2966.889454	836590.020605	40.017383
2970.265013	838198.588676	40.022400
2972.781265	839832.199460	40.027418
2976.092873	841443.319911	40.032436
2978.952786	843061.062297	40.037453
2981.466157	844686.034938	40.042471
2984.435671	846316.445680	40.047488
2987.192550	847964.160298	40.052506
2990.242596	849597.984027	40.057524
2992.989562	851240.466194	40.062541
2995.556332	852904.398645	40.067559
2999.033661	854562.686583	40.072576
3001.868493	856212.870639	40.077594
3004.386191	857877.999273	40.082612
3007.371972	859521.158700	40.087629
3010.284340	861167.381736	40.092647
3013.843625	862775.043065	40.097664
3016.415707	864406.678486	40.102682
3019.414142	866037.999036	40.107700
3022.769979	867659.034950	40.112717
3025.416646	869291.182015	40.117735
3028.609276	870896.649627	40.122752
3031.473437	872546.855696	40.127770
3034.445792	874191.651903	40.132788
3037.904837	875834.268502	40.137805
3040.619164	877467.266685	40.142823
3043.408694	879119.142482	40.147840
3046.461886	880780.856332	40.152858
3049.697930	882436.947478	40.157876
3052.918060	884105.906654	40.162893
3055.842721	885786.125065	40.167911
3059.045185	887452.196302	40.172928
3061.893106	889118.812389	40.177946
3065.087647	890804.964845	40.182964
3068.434105	892501.500945	40.187981
3071.143968	894181.821814	40.192999
3074.288442	895867.459348	40.198016
3077.417811	897576.121687	40.203034
3080.458227	899276.864392	40.208052
3083.729845	900975.902012	40.213069
3087.113324	902710.910860	40.218087
3089.741371	904433.281306	40.223104
3092.697354	906147.945909	40.228122
3095.590208	907875.084281	40.233140
3098.603550	909617.634510	40.238157
3101.479571	911374.757085	40.243175
3104.395808	913121.509411	40.248192
3107.734301	914882.053179	40.253210
3110.588606	916634.714977	40.258228
3113.845255	918394.912265	40.263245
3116.231083	920193.087000	40.268263
3119.548356	921970.071014	40.273280
3122.985117	923752.976298	40.278298
3126.014077	925548.883053	40.283316
3129.518406	927345.262335	40.288333
3132.785801	929147.979390	40.293351
3135.876101	930941.206497	40.298368
3139.166787	932737.244537	40.303386
3142.219638	934539.320215	40.308404
3145.507758	936331.075460	40.313421
3148.523636	938133.460999	40.318439
3151.533440	939938.672101	40.323456
3154.457910	941774.349778	40.328474
3157.663031	943579.799675	40.333492
3161.137352	945393.559446	40.338509
3163.644755	947219.260133	40.343527
3166.719133	949047.754247	40.348544
3170.625276	950878.992602	40.353562
3173.353601	952716.735566	40.358580
3177.010492	954547.655183	40.363597
3180.113368	956449.790242	40.368615
3183.255825	958330.514972	40.373632
3186.474438	960204.747990	40.378650
3189.509333	962097.656556	40.383668
3192.608329	963969.121105	40.388685
3195.909666	965865.632310	40.393703
3199.081328	967754.606835	40.398720
3202.194431	969642.579569	40.403738
3205.335902	971540.465204	40.408756
3208.585009	973431.072035	40.413773
3211.991241	975335.168754	40.418791
3215.059987	977220.263915	40.423808
3218.614216	979102.026834	40.428826
3221.494630	980963.700325	40.433844
3224.818181	982793.725216	40.438861
3227.744392	984646.204399	40.443879
3230.872882	986486.758893	40.448896
3234.146330	988341.677744	40.453914
3236.712996	990190.175636	40.458932
3240.274206	992036.061563	40.463949
3243.456640	993906.195298	40.468967
3246.255762	995791.128062	40.473984
3249.254270	997671.807752	40.479002
3252.229658	999554.100448	40.484020
3255.449434	1001462.032359	40.489037
3258.396088	1003377.710729	40.494055
3261.747174	1005301.985335	40.499072
3264.913935	1007221.949814	40.504090
3267.825511	1009155.358537	40.509108
3271.120218	1011099.378523	40.514125
3273.979392	1013045.995856	40.519143
3277.254372	1015010.753955	40.524160
3280.527861	1016984.118431	40.529178
3283.646987	1018970.942807	40.534196
3287.057366	1020945.407969	40.539213
3290.268518	1022941.354231	40.544231
3293.601076	1024945.752187	40.549248
3297.075891	1026946.896403	40.554266
3300.502362	1028953.031248	40.559284
3303.945950	1030970.222820	40.564301
3307.731420	1032985.760123	40.569319
3311.206284	1034982.962374	40.574336
3314.405241	1037001.774747	40.579354
3317.862069	1039032.828720	40.584372
3320.896169	1041047.210544	40.589389
3323.956793	1043081.186929	40.594407
3327.398612	1045119.170561	40.599424
3330.598942	1047159.814363	40.604442
3333.845146	1049210.958943	40.609460
3336.762746	1051263.417506	40.614477
3339.944681	1053334.015921	40.619495
3342.826666	1055409.751449	40.624512
3346.423793	1057481.320807	40.629530
3349.573385	1059573.030448	40.634548
3352.846969	1061663.156751	40.639565
3356.026823	1063770.933903	40.644583
3359.595561	1065863.061917	40.649600
3362.830271	1067972.479446	40.654618
3366.060471	1070098.344199	40.659636
3369.363154	1072213.979670	40.664653
3372.728830	1074332.139960	40.669671
3375.946293	1076453.334595	40.674688
3379.747527	1078587.106946	40.679706
3382.847722	1080733.078453	40.684724
3385.955683	1082867.107959	40.689741
3389.648737	1085007.853942	40.694759
3392.978244	1087151.831454	40.699776
3396.196911	1089307.401456	40.704794
3399.919164	1091465.757060	40.709812
3403.376764	1093620.624052	40.714829
3406.992999	1095771.076860	40.719847
3410.173937	1097931.334770	40.724864
3414.208863	1100067.704645	40.729882
3417.841845	1102208.346957	40.734900
3421.379203	1104334.912271	40.739917
3424.982695	1106472.341618	40.744935
3428.648782	1108606.436735	40.749952
3431.873186	1110723.389800	40.754970
3435.340983	1112854.307938	40.759988
3438.658150	1114994.769120	40.765005
3442.457154	1117106.171209	40.770010
3445.291635	1119150.657210	40.775015
3448.705653	1121149.132509	40.780020
3451.599596	1123097.259783	40.785024
3454.849262	1124953.272596	40.790029
3458.125497	1126738.437064	40.795034
3460.441682	1128459.547257	40.800039
3463.661076	1130094.303936	40.805044
3466.449644	1131664.387926	40.810048
3468.814389	1133158.169235	40.815053
3471.135236	1134555.988318	40.820058
3473.684425	1135906.208706	40.825063
3476.246489	1137174.536011	40.830068
3478.215074	1138370.050316	40.835072
3480.688613	1139498.882682	40.840077
3482.775488	1140570.899358	40.845082
3484.873729	1141570.797570	40.850087
3487.083090	1142482.858465	40.855092
3488.250235	1143369.616097	40.860096
3490.109903	1144177.989669	40.865101
3492.221679	1144927.615279	40.870106
3493.651685	1145628.813348	40.875111
3494.956765	1146280.848062	40.880116
3496.515257	1146881.306310	40.885120
3497.932067	1147423.638239	40.890125
3499.284458	1147941.576754	40.895130
3500.299962	1148395.197005	40.900135
3501.696503	1148816.509147	40.905140
3502.308060	1149203.060834	40.910144
3503.314378	1149552.865923	40.915149
3504.464296	1149865.688958	40.920154
3505.557285	1150143.084758	40.925159
3506.206194	1150384.743893	40.930164
3507.226609	1150620.649215	40.935168
3508.112121	1150800.226466	40.940173
3508.742186	1150957.588429	40.945178
3509.188809	1151087.991047	40.950183
3510.086244	1151198.811749	40.955188
3510.707686	1151282.881076	40.960192
3511.197690	1151340.365865	40.965197
3512.279158	1151377.491413	40.970202
3512.364577	1151387.134675	40.975207
3513.213856	1151390.024630	40.980212
3513.694768	1151377.542642	40.985216
3514.232283	1151329.357227	40.990221
3514.970299	1151265.610738	40.995226
3514.952125	1151201.893334	41.000231
3515.729224	1151084.169283	41.005236
3515.728447	1150977.080858	41.010240
3516.260465	1150864.599990	41.015245
3516.556199	1150730.945049	41.020250
3516.860260	1150583.365500	41.025255
3517.061770	1150425.950355	41.030260
3517.330562	1150265.394373	41.035264
3517.656574	1150095.353914	41.040269
3518.107624	1149903.694642	41.045274
3518.285491	1149702.602526	41.050279
3518.823075	1149490.740986	41.055284
3518.682328	1149275.762293	41.060288
3518.885349	1149043.100209	41.065293
3519.190305	1148814.010615	41.070298
3519.223131	1148575.198808	41.075303
3519.603562	1148331.866473	41.080308
3519.758322	1148075.486254	41.085312
3519.886873	1147825.445645	41.090317
3519.875763	1147555.708776	41.095322
3520.114217	1147285.064249	41.100327
3520.304854	1146994.609456	41.105332
3520.187614	1146725.037126	41.110336
3520.262855	1146438.645524	41.115341
3520.559198	1146146.705165	41.120346
3520.399333	1145862.216472	41.125351
3520.772171	1145560.374213	41.130356
3520.788693	1145272.981237	41.135360
3521.081874	1144960.311938	41.140365
3520.991058	1144652.996152	41.145370
3520.906676	1144351.634141	41.150375
3520.928124	1144033.550883	41.155380
3521.059630	1143711.637708	41.160384
3521.118549	1143377.674466	41.165389
3521.271255	1143071.079995	41.170394
3520.937889	1142762.556302	41.175399
3521.076509	1142418.087658	41.180404
3521.199346	1142096.551793	41.185408
3521.210695	1141766.288447	41.190413
3521.460713	1141423.159455	41.195418
3521.376857	1141102.356084	41.200423
3521.504089	1140765.655382	41.205428
3521.352511	1140419.871163	41.210432
3521.328257	1140068.635141	41.215437
3521.742112	1139745.864858	41.220442
3521.362676	1139398.533275	41.225447
3521.715573	1139044.130611	41.230452
3521.553368	1138707.251816	41.235456
3521.503153	1138359.038615	41.240461
3521.797993	1138008.847340	41.245466
3521.337500	1137655.434965	41.250471
3521.541622	1137298.092321	41.255476
3521.436833	1136968.118444	41.260480
3521.531038	1136622.900355	41.265485
3521.882346	1136257.488129	41.270490
3521.477550	1135898.537342	41.275495
3521.631769	1135535.671693	41.280500
3521.405114	1135193.072381	41.285504
3521.420484	1134826.952210	41.290509
3521.655229	1134467.704346	41.295514
3521.276207	1134115.182443	41.300519
3521.606103	1133757.675662	41.305524
3521.502791	1133398.316154	41.310528
3521.694550	1133040.403862	41.315533
3521.638262	1132683.078402	41.320538
3521.691369	1132323.905519	41.325543
3521.995244	1131963.621778	41.330548
3521.430448	1131598.800069	41.335552
3521.570849	1131230.700870	41.340557
3521.475826	1130865.656453	41.345562
3521.699543	1130498.253224	41.350567
3521.259303	1130138.063427	41.355572
3521.291474	1129779.862885	41.360576
3521.243453	1129405.108881	41.365581
3521.466688	1129037.129510	41.370586
3521.063810	1128688.054720	41.375591
3521.555440	1128313.515356	41.380596
3521.244866	1127961.334789	41.385600
3521.097811	1127592.365601	41.390605
3521.252404	1127231.881191	41.395610
3521.299390	1126865.302593	41.400615
3521.000004	1126495.521605	41.405620
3521.193083	1126148.370091	41.410624
3521.110682	1125762.901131	41.415629
3521.145157	1125395.652721	41.420634
3520.905655	1125044.409400	41.425639
3521.197956	1124677.449689	41.430644
3521.031417	1124309.874171	41.435648
3520.944285	1123945.971876	41.440653
3521.276219	1123586.353861	41.445658
3521.015291	1123222.430867	41.450663
3520.802057	1122852.002344	41.455668
3520.918466	1122487.871952	41.460672
3521.239066	1122116.638143	41.465677
3520.674438	1121763.709217	41.470682
3520.824998	1121400.832037	41.475687
3520.864206	1121030.997379	41.480692
3520.637624	1120680.797900	41.485696
3520.449892	1120310.665097	41.490701
3520.656781	1119942.917949	41.495706
3520.412019	1119584.935151	41.500711
3520.512070	1119230.872262	41.505716
3520.460608	1118879.668697	41.510720
3520.775058	1118509.900131	41.515725
3520.711612	1118145.122464	41.520730
3520.222908	1117801.160881	41.525735
3520.648398	1117423.771946	41.530740
3520.246133	1117057.451388	41.535744
3520.345317	1116695.216335	41.540749
3520.110479	1116342.161103	41.545754
3520.113155	1115991.045024	41.550759
3520.593392	1115622.956037	41.555764
3520.241021	1115271.660664	41.560768
3520.082402	1114909.442669	41.565773
3520.365072	1114551.513027	41.570778
3520.060209	1114198.900144	41.575783
3520.403628	1113835.287445	41.580788
3520.108711	1113481.672270	41.585792
3519.465713	1113113.405290	41.590797
3519.926632	1112767.056808	41.595802
3519.783185	1112420.785517	41.600807
3519.682441	1112058.556196	41.605812
3519.646358	1111706.307490	41.610816
3519.595355	1111352.130255	41.615821
3519.726800	1111006.771821	41.620826
3519.540353	1110652.379949	41.625831
3519.396316	1110290.324699	41.630836
3519.554383	1109948.137862	41.635840
3519.399751	1109600.827794	41.640845
3519.568167	1109252.774060	41.645850
3519.188626	1108908.319219	41.650855
3519.084162	1108563.510672	41.655860
3519.347153	1108211.842579	41.660864
3519.254917	1107870.423769	41.665869
3519.213620	1107522.483498	41.670874
3518.883554	1107188.124725	41.675879
3519.069400	1106842.776191	41.680884
3518.830347	1106509.219510	41.685888
3518.579691	1106163.803823	41.690893
3519.082446	1105819.483286	41.695898
3518.800173	1105482.718883	41.700903
3519.070767	1105139.157080	41.705908
3518.936598	1104805.668594	41.710912
3518.898219	1104452.658400	41.715917
3519.081859	1104096.913883	41.720922
3518.524939	1103769.353273	41.725927
3518.673389	1103421.785427	41.730932
3518.868844	1103084.123661	41.735936
3518.750918	1102742.383864	41.740941
3518.544898	1102405.892310	41.745946
3518.750715	1102075.427675	41.750951
3518.912744	1101734.437934	41.755956
3518.736003	1101383.351959	41.760960
3518.461717	1101042.677074	41.765965
3518.779876	1100711.441374	41.770970
3518.464908	1100378.760212	41.775975
3518.547955	1100031.175851	41.780980
3518.204352	1099692.817050	41.785984
3518.066403	1099356.888945	41.790989
3518.441891	1099026.783359	41.795994
3518.052505	1098687.795459	41.800999
3518.375744	1098361.291325	41.806004
3518.125349	1098032.184305	41.811008
3518.072146	1097695.756441	41.816013
3517.892600	1097360.380507	41.821018
3517.697962	1097036.750920	41.826023
3518.224903	1096714.322269	41.831028
3518.357686	1096381.990779	41.836032
3517.946210	1096038.535688	41.841037
3517.805939	1095709.077786	41.846042
3517.626871	1095394.244756	41.851047
3517.395585	1095063.997153	41.856052
3517.690952	1094737.852945	41.861056
3517.503341	1094413.395436	41.866061
3517.406933	1094092.061549	41.871066
3517.076298	1093781.179040	41.876071
3517.275939	1093451.240610	41.881076
3517.404303	1093139.671421	41.886080
3517.381241	1092821.695881	41.891085
3517.280415	1092492.992974	41.896090
3516.721495	1092184.545348	41.901095
3517.229857	1091876.191603	41.906100
3517.106057	1091551.552153	41.911104
3517.166815	1091236.437884	41.916109
3517.089167	1090910.890726	41.921114
3517.280668	1090605.389593	41.926119
3517.032530	1090280.407240	41.931124
3516.954901	1089969.551674	41.936128
3516.894417	1089653.982355	41.941133
3516.952846	1089342.398010	41.946138
3516.574720	1089034.795026	41.951143
3516.829382	1088718.640478	41.956148
3516.790865	1088411.329413	41.961152
3516.675033	1088096.540865	41.966157
3516.751760	1087780.456813	41.971162
3516.484004	1087479.645929	41.976167
3516.585996	1087170.420997	41.981172
3516.392841	1086869.755699	41.986176
3516.472180	1086562.799773	41.991181
3516.530748	1086259.184261	41.996186
3516.331453	1085962.590813	42.001191
3516.479278	1085649.342223	42.006196
3516.655348	1085352.174415	42.011200
3516.201324	1085036.593301	42.016205
3516.615187	1084732.067129	42.021210
3516.395601	1084434.818500	42.026215
3516.407655	1084126.777436	42.031220
3516.215088	1083821.629059	42.036224
3515.989878	1083527.016420	42.041229
3515.796848	1083219.628983	42.046234
3515.846167	1082921.198571	42.051239
3516.039180	1082625.509293	42.056244
3516.144433	1082336.531911	42.061248
3515.814140	1082025.167453	42.066253
3516.251620	1081727.374995	42.071258
3515.879136	1081429.891510	42.076263
3515.865508	1081120.533491	42.081268
3515.851056	1080825.835908	42.086272
3515.764305	1080540.920045	42.091277
3515.989333	1080232.047922	42.096282
3515.876087	1079941.156541	42.101287
3515.837299	1079641.793391	42.106292
3516.041937	1079347.459579	42.111296
3515.832188	1079054.617604	42.116301
3516.037148	1078757.181017	42.121306
3515.555778	1078470.302542	42.126311
3515.328447	1078168.778141	42.131316
3515.559243	1077878.967850	42.136320
3515.660551	1077590.411376	42.141325
3515.276393	1077286.752277	42.146330
3515.150073	1077005.210051	42.151335
3515.316132	1076708.820245	42.156340
3515.419870	1076440.459828	42.161344
3515.213893	1076142.564393	42.166349
3515.565621	1075849.746001	42.171354
3515.106101	1075562.807101	42.176359
3515.120748	1075271.453626	42.181364
3515.034076	1074982.502214	42.186368
3514.906865	1074694.790739	42.191373
3514.976236	1074411.449878	42.196378
3515.109445	1074139.321820	42.201383
3515.243528	1073856.709966	42.206388
3514.951422	1073577.131593	42.211392
3514.793884	1073289.255080	42.216397
3515.068516	1073003.021520	42.221402
3515.022052	1072724.127654	42.226407
3514.906796	1072436.295366	42.231412
3514.796983	1072160.169537	42.236416
3514.705020	1071881.528474	42.241421
3514.982902	1071597.238758	42.246426
3514.721490	1071330.032919	42.251431
3514.374832	1071037.936770	42.256436
3514.212015	1070772.129043	42.261440
3514.222809	1070504.934210	42.266445
3514.281497	1070228.298717	42.271450
3514.227062	1069968.681931	42.276455
3514.189809	1069689.247411	42.281460
3514.386925	1069418.412111	42.286464
3513.898612	1069155.175138	42.291469
3514.095238	1068885.082674	42.296474
3514.148536	1068617.596508	42.301479
3514.179238	1068354.908651	42.306484
3514.435918	1068075.920381	42.311488
3514.243675	1067817.089780	42.316493
3514.240186	1067533.597149	42.321498
3513.834699	1067269.486626	42.326503
3513.670802	1067010.228585	42.331508
3513.863359	1066753.496465	42.336512
3513.745527	1066490.839965	42.341517
3513.736104	1066223.535915	42.346522
3513.793400	1065975.831554	42.351527
3513.840061	1065706.953999	42.356532
3513.656366	1065456.764728	42.361536
3513.856617	1065188.702329	42.366541
3513.980311	1064936.225924	42.371546
3513.570288	1064676.705748	42.376551
3513.333722	1064415.701409	42.381556
3513.357255	1064165.515391	42.386560
3513.153304	1063904.481387	42.391565
3513.675537	1063658.135592	42.396570
3513.541867	1063398.220782	42.401575
3512.889180	1063132.219531	42.406580
3513.252518	1062882.304100	42.411584
3513.342172	1062631.363603	42.416589
3512.847023	1062385.705865	42.421594
3512.944891	1062144.560032	42.426599
3513.132840	1061880.092431	42.431604
3512.968524	1061640.122855	42.436608
3513.115749	1061399.417576	42.441613
3513.303135	1061139.728200	42.446618
3512.913947	1060888.883334	42.451623
3512.978447	1060648.255100	42.456628
3513.456310	1060406.007596	42.461632
3512.932282	1060153.418148	42.466637
3513.162712	1059900.789146	42.471642
3512.525454	1059662.448305	42.476647
3513.112564	1059408.389697	42.481652
3512.994116	1059166.956363	42.486656
3512.620435	1058928.925602	42.491661
3512.858375	1058669.496624	42.496666
3512.772177	1058429.566806	42.501671
3512.784779	1058195.293774	42.506676
3512.773525	1057949.743536	42.511680
3512.527470	1057708.363610	42.516685
3512.672542	1057462.091521	42.521690
3512.686239	1057226.813697	42.526695
3512.456708	1056980.678142	42.531700
3512.543033	1056732.167024	42.536704
3512.389159	1056512.688710	42.541709
3512.657530	1056269.619283	42.546714
3512.345463	1056042.246418	42.551719
3512.376097	1055791.774726	42.556724
3512.246681	1055551.919479	42.561728
3512.350740	1055322.328106	42.566733
3512.418236	1055080.106774	42.571738
3512.071207	1054852.401454	42.576743
3512.398519	1054602.116054	42.581748
3512.269982	1054386.115489	42.586752
3512.095703	1054157.003457	42.591757
3512.236427	1053924.841472	42.596762
3512.126340	1053695.603311	42.601767
3512.061868	1053462.009520	42.606772
3512.055623	1053230.131770	42.611776
3511.898810	1053011.189535	42.616781
3512.056112	1052770.587640	42.621786
3512.133447	1052553.035061	42.626791
3511.871042	1052322.704268	42.631796
3511.792387	1052081.821938	42.636800
3511.930010	1051854.684618	42.641805
3512.074017	1051633.902301	42.646810
3512.074058	1051416.703491	42.651815
3511.878564	1051182.456177	42.656820
3511.815078	1050949.334679	42.661824
3511.789841	1050732.498974	42.666829
3512.023129	1050487.637343	42.671834
3511.587120	1050263.616006	42.676839
3511.271409	1050047.669505	42.681844
3511.668388	1049835.070349	42.686848
3511.605781	1049613.373082	42.691853
3511.550225	1049386.552095	42.696858
3511.445377	1049179.799475	42.701863
3511.435970	1048957.295248	42.706868
3511.061446	1048743.140840	42.711872
3511.139035	1048527.166689	42.716877
3511.294202	1048312.039864	42.721882
3510.786849	1048101.935645	42.726887
3511.204749	1047873.334034	42.731892
3511.342196	1047656.930031	42.736896
3511.097396	1047453.900044	42.741901
3511.567448	1047233.274428	42.746906
3511.718812	1047018.677113	42.751911
3511.243761	1046802.147534	42.756916
3511.408352	1046577.974538	42.761920
3511.211781	1046370.552883	42.766925
3511.635485	1046155.394588	42.771930
3510.926672	1045943.117711	42.776935
3510.868634	1045718.753528	42.781940
3511.347259	1045504.429854	42.786945
3510.506992	1045305.570916	42.791949
3510.919173	1045092.497482	42.796954
3510.941404	1044891.067634	42.801959
3511.064185	1044674.646112	42.806964
3510.799179	1044458.086871	42.811969
3510.483340	1044259.683442	42.816973
3510.826627	1044053.534748	42.821978
3510.826624	1043851.781076	42.826983
3510.684345	1043639.612374	42.831988
3511.057253	1043440.583283	42.836993
3510.675919	1043231.529161	42.841997
3510.680100	1043021.147925	42.847002
3510.670359	1042823.029065	42.852007
3510.636563	1042619.497367	42.857012
3510.609081	1042412.286140	42.862017
3510.692174	1042211.521801	42.867021
3510.866784	1042007.160451	42.872026
3510.443651	1041814.677232	42.877031
3510.644180	1041600.151908	42.882036
3510.891421	1041401.843380	42.887041
3510.417647	1041197.462393	42.892045
3510.684630	1040990.826005	42.897050
3510.376453	1040781.474265	42.902055
3510.663962	1040584.289530	42.907060
3510.495534	1040388.525867	42.912065
3510.308998	1040186.186454	42.917069
3510.535540	1039978.359337	42.922074
3510.493491	1039788.642560	42.927079
3510.408849	1039589.550791	42.932084
3510.280162	1039386.882777	42.937089
3510.777176	1039191.450636	42.942093
3510.568842	1038993.034506	42.947098
3510.084437	1038789.726646	42.952103
3510.303494	1038589.969042	42.957108
3510.442665	1038392.537642	42.962113
3510.100998	1038201.559257	42.967117
3510.466737	1038007.170596	42.972122
3510.266262	1037810.257880	42.977127
3509.958012	1037613.452630	42.982132
3510.137394	1037430.967313	42.987137
3510.224109	1037230.602536	42.992141
3510.194994	1037027.832132	42.997146
3510.065412	1036837.642274	43.002151
3510.382361	1036635.090674	43.007156
3510.310996	1036448.262645	43.012161
3509.894663	1036256.939652	43.017165
3510.426375	1036057.329764	43.022170
3510.160063	1035855.522880	43.027175
3509.797699	1035674.326553	43.032180
3510.146724	1035489.234838	43.037185
3509.677294	1035289.085218	43.042189
3509.761332	1035101.606020	43.047194
3510.044027	1034915.635574	43.052199
3509.762317	1034730.622534	43.057204
3509.877559	1034538.379006	43.062209
3509.429595	1034352.800338	43.067213
3509.845180	1034165.622022	43.072218
3509.425632	1033989.314487	43.077223
3509.940211	1033796.689345	43.082228
3509.692907	1033613.181615	43.087233
3509.035096	1033421.800954	43.092237
3509.456726	1033242.138081	43.097242
3509.307767	1033061.692482	43.102247
3509.314535	1032871.925312	43.107252
3509.396544	1032706.816873	43.112257
3509.163224	1032531.884168	43.117261
3509.221863	1032357.381791	43.122266
3509.006652	1032174.305301	43.127271
3509.316657	1031991.426659	43.132276
3509.353408	1031825.234918	43.137281
3509.439940	1031651.964149	43.142285
3509.607774	1031464.735979	43.147290
3509.218740	1031287.660372	43.152295
3509.207615	1031108.000041	43.157300
3509.386748	1030930.141894	43.162305
3509.347948	1030756.767163	43.167309
3509.139673	1030572.668878	43.172314
3509.503242	1030399.216772	43.177319
3509.366363	1030220.419913	43.182324
3509.504925	1030044.186123	43.187329
3508.780754	1029871.284048	43.192333
3509.347922	1029696.421048	43.197338
3509.477111	1029523.270820	43.202343
3509.369114	1029329.819357	43.207348
3509.160830	1029163.395038	43.212353
3509.296164	1028995.650259	43.217357
3509.536137	1028808.999009	43.222362
3509.131763	1028625.740392	43.227367
3508.863804	1028453.590868	43.232372
3509.297392	1028277.059032	43.237377
3508.949805	1028104.233896	43.242381
3509.097527	1027936.358420	43.247386
3508.979842	1027761.838252	43.252391
3508.909473	1027579.071447	43.257396
3509.218412	1027419.387288	43.262401
3508.773029	1027247.907898	43.267405
3508.611580	1027065.139288	43.272410
3508.786537	1026904.396891	43.277415
3508.837851	1026738.051311	43.282420
3508.937959	1026562.198401	43.287425
3508.731085	1026394.625674	43.292429
3508.947387	1026230.756817	43.297434
3509.011058	1026074.465693	43.302439
3508.914855	1025895.523687	43.307444
3508.751206	1025714.455357	43.312449
3508.562736	1025559.547915	43.317453
3508.935621	1025391.268247	43.322458
3508.741474	1025232.864241	43.327463
3508.761612	1025045.735934	43.332468
3508.894060	1024887.268355	43.337473
3508.483756	1024730.339374	43.342477
3508.411054	1024560.266766	43.347482
3508.683215	1024407.577542	43.352487
3508.442433	1024237.425889	43.357492
3508.665211	1024073.880490	43.362497
3508.495794	1023913.981212	43.367501
3508.350518	1023741.375573	43.372506
3508.225908	1023588.147774	43.377511
3508.102813	1023427.063766	43.382516
3508.002535	1023276.537623	43.387521
3508.304114	1023123.420790	43.392525
3508.729624	1022957.482827	43.397530
3508.614675	1022809.564028	43.402535
3508.170462	1022650.061697	43.407540
3508.118890	1022487.872459	43.412545
3507.642013	1022323.906436	43.417549
3508.097334	1022172.968266	43.422554
3507.898370	1022025.139546	43.427559
3507.779617	1021877.099790	43.432564
3507.618335	1021716.651615	43.437569
3507.804530	1021583.680409	43.442573
3508.065541	1021433.820986	43.447578
3507.925029	1021287.029836	43.452583
3507.601271	1021124.555048	43.457588
3508.179021	1020979.092167	43.462593
3507.835970	1020830.479841	43.467597
3507.840953	1020683.648928	43.472602
3507.754519	1020527.518616	43.477607
3507.929398	1020379.972872	43.482612
3508.305826	1020236.075698	43.487617
3507.638018	1020081.483578	43.492621
3508.194300	1019929.304478	43.497626
3507.964195	1019796.941448	43.502631
3507.737457	1019632.661473	43.507636
3507.796269	1019479.485097	43.512641
3507.470019	1019330.927257	43.517645
3507.457855	1019196.671045	43.522650
3507.681368	1019052.283658	43.527655
3507.931520	1018899.253953	43.532660
3507.998488	1018758.571318	43.537665
3507.727118	1018618.425974	43.542669
3507.636198	1018472.038059	43.547674
3507.393345	1018310.923731	43.552679
3507.635848	1018178.638725	43.557684
3507.885314	1018032.862481	43.562689
3507.468725	1017882.534650	43.567693
3507.822383	1017730.620422	43.572698
3507.520428	1017599.866966	43.577703
3507.655881	1017452.541856	43.582708
3507.655213	1017307.079087	43.587713
3507.599951	1017157.351614	43.592717
3507.772431	1017019.325248	43.597722
3507.520231	1016872.048760	43.602727
3507.552860	1016720.936495	43.607732
3507.507603	1016577.306147	43.612737
3507.295133	1016446.025811	43.617741
3507.677630	1016306.006210	43.622746
3507.618772	1016164.017533	43.627751
3507.481914	1016016.602557	43.632756
3507.464223	1015868.484623	43.637761
3507.180134	1015744.673780	43.642765
3507.081722	1015596.561974	43.647770
3507.072002	1015460.565816	43.652775
3506.822900	1015313.830401	43.657780
3507.247157	1015189.016969	43.662785
3506.940959	1015059.467072	43.667789
3507.263468	1014915.830767	43.672794
3506.995762	1014789.763286	43.677799
3507.042455	1014653.641232	43.682804
3506.972145	1014518.214781	43.687809
3506.874839	1014389.683026	43.692813
3507.026658	1014257.126452	43.697818
3507.053506	1014140.608194	43.702823
3507.157270	1014006.305897	43.707828
3507.098350	1013868.337365	43.712833
3507.031879	1013740.174091	43.717837
3507.149190	1013606.928162	43.722842
3507.018986	1013472.651661	43.727847
3506.670502	1013338.505015	43.732852
3506.907910	1013204.452896	43.737857
3506.679516	1013088.149102	43.742861
3506.750657	1012953.244358	43.747866
3506.666051	1012831.958644	43.752871
3506.581033	1012709.990540	43.757876
3506.932492	1012577.750006	43.762881
3506.720209	1012451.426726	43.767885
3506.827405	1012316.500784	43.772890
3506.818760	1012201.113736	43.777895
3506.789402	1012076.888769	43.782900
3506.983646	1011937.277086	43.787905
3506.314083	1011813.831693	43.792909
3506.610541	1011685.464709	43.797914
3506.766403	1011573.923246	43.802919
3506.777576	1011440.934944	43.807924
3506.587354	1011312.251042	43.812929
3506.444213	1011187.442323	43.817933
3506.508803	1011076.197477	43.822938
3506.587363	1010958.827633	43.827943
3506.545089	1010830.302652	43.832948
3506.855322	1010700.356508	43.837953
3506.477124	1010583.442693	43.842957
3507.030227	1010460.252022	43.847962
3506.776112	1010342.049686	43.852967
3506.620416	1010222.857025	43.857972
3506.803700	1010086.116175	43.862977
3506.397498	1009966.182014	43.867981
3506.151669	1009829.214101	43.872986
3506.388931	1009735.599322	43.877991
3506.603869	1009616.624308	43.882996
3506.564625	1009486.124687	43.888001
3506.291297	1009364.989726	43.893005
3506.513194	1009253.780172	43.898010
3506.290840	1009141.086680	43.903015
3506.611069	1009021.498675	43.908020
3506.600488	1008889.425572	43.913025
3506.263292	1008770.232077	43.918029
3506.392360	1008640.754240	43.923034
3506.163980	1008519.204934	43.928039
3506.481442	1008408.060158	43.933044
3506.345418	1008299.612195	43.938049
3506.296245	1008183.177553	43.943053
3506.516692	1008058.142432	43.948058
3506.250440	1007954.083309	43.953063
3506.139966	1007829.486433	43.958068
3506.091260	1007707.112390	43.963073
3505.777278	1007600.818849	43.968077
3506.073295	1007489.465096	43.973082
3506.040986	1007379.524197	43.978087
3506.058246	1007264.128981	43.983092
3506.359523	1007143.823799	43.988097
3505.879795	1007043.088389	43.993101
3505.962663	1006929.328233	43.998106
3506.293363	1006808.913847	44.003111
3506.224691	1006694.882258	44.008116
3506.291615	1006577.812016	44.013121
3505.929358	1006477.630517	44.018125
3505.946583	1006365.230997	44.023130
3505.782773	1006258.012347	44.028135
3505.845600	1006158.921960	44.033140
3506.050919	1006040.456510	44.038145
3505.780382	1005944.528805	44.043149
3506.297842	1005824.646098	44.048154
3505.977908	1005707.427044	44.053159
3505.874623	1005599.407985	44.058164
3505.671060	1005502.392058	44.063169
3505.426690	1005398.865662	44.068173
3505.881482	1005272.563279	44.073178
3505.286933	1005171.521609	44.078183
3505.624612	1005082.383865	44.083188
3505.755724	1004972.369164	44.088193
3505.579091	1004872.809379	44.093197
3505.904977	1004766.551563	44.098202
3505.751173	1004669.026835	44.103207
3505.820030	1004556.874594	44.108212
3505.940655	1004446.073285	44.113217
3505.740904	1004348.842385	44.118221
3505.893436	1004234.821941	44.123226
3505.807137	1004134.747935	44.128231
3505.642530	1004022.526272	44.133236
3505.839688	1003917.732759	44.138241
3505.825156	1003817.154948	44.143245
3505.754047	1003703.549717	44.148250
3505.904240	1003594.380530	44.153255
3505.468565	1003500.481327	44.158260
3505.676025	1003395.773722	44.163265
3505.414729	1003282.580476	44.168269
3505.777957	1003185.139543	44.173274
3505.440216	1003087.715097	44.178279
3505.328193	1002989.668064	44.183284
3505.571507	1002880.664337	44.188289
3505.332189	1002786.818221	44.193293
3505.616219	1002683.155018	44.198298
3505.373016	1002592.906178	44.203303
3505.321871	1002495.813505	44.208308
3505.603273	1002404.307692	44.213313
3505.246310	1002294.807751	44.218317
3505.629721	1002195.886955	44.223322
3505.857208	1002103.995960	44.228327
3505.329158	1001990.820780	44.233332
3505.627965	1001883.734810	44.238337
3505.327834	1001797.666858	44.243341
3505.384312	1001708.522246	44.248346
3505.307487	1001602.271298	44.253351
3505.417255	1001504.648547	44.258356
3505.386758	1001403.738491	44.263361
3505.165824	1001321.932130	44.268365
3505.654870	1001222.198386	44.273370
3505.795764	1001124.174672	44.278375
3505.196611	1001023.254168	44.283380
3505.800151	1000917.462236	44.288385
3505.503044	1000842.182173	44.293389
3505.611878	1000712.623200	44.298394
3505.499379	1000625.435904	44.303399
3505.066906	1000537.813312	44.308404
3505.424722	1000423.390221	44.313409
3505.048852	1000341.887201	44.318413
3505.539797	1000244.179931	44.323418
3505.306518	1000143.475471	44.328423
3504.932053	1000053.305055	44.333428
3505.373586	999949.371162	44.338433
3505.130115	999868.034191	44.343437
3505.167819	999771.366834	44.348442
3504.847080	999672.712615	44.353447
3505.060674	999594.022091	44.358452
3505.349234	999495.264428	44.363457
3504.991210	999410.921959	44.368461
3504.894264	999319.136541	44.373466
3504.965414	999232.286943	44.378471
3504.941072	999139.707837	44.383476
3505.080568	999050.994470	44.388481
3505.200902	998962.867014	44.393485
3505.365642	998867.623671	44.398490
3505.095162	998769.334866	44.403495
3504.919585	998688.456567	44.408500
3504.971546	998604.521367	44.413505
3505.036456	998511.430476	44.418509
3504.949827	998408.918433	44.423514
3504.825067	998329.195036	44.428519
3504.802671	998248.382591	44.433524
3505.243073	998156.295089	44.438529
3505.005438	998068.407423	44.443533
3505.129152	997976.466533	44.448538
3505.340367	997893.857819	44.453543
3505.303626	997791.618519	44.458548
3505.031770	997700.322565	44.463553
3505.054717	997613.261332	44.468557
3505.056963	997511.789606	44.473562
3505.239904	997428.204943	44.478567
3505.201521	997328.781692	44.483572
3505.293593	997235.081051	44.488577
3505.198679	997147.739920	44.493581
3505.131079	997044.518340	44.498586
3505.077428	996969.536226	44.503591
3505.098339	996879.347524	44.508596
3505.439210	996777.514706	44.513601
3505.005841	996696.163448	44.518605
3504.771625	996597.538797	44.523610
3505.391504	996514.063493	44.528615
3505.340016	996429.918332	44.533620
3505.179415	996325.043156	44.538625
3505.254829	996243.504200	44.543629
3505.184103	996143.383660	44.548634
3505.203715	996045.681662	44.553639
3504.983334	995954.543919	44.558644
3505.196800	995864.599594	44.563649
3504.996148	995773.650516	44.568653
3504.845098	995683.081464	44.573658
3505.034890	995593.039320	44.578663
3505.215455	995514.687274	44.583668
3505.058062	995414.762980	44.588673
3505.138532	995327.852021	44.593677
3505.446837	995232.523967	44.598682
3505.151088	995148.984560	44.603687
3504.980827	995056.460210	44.608692
3505.064162	994962.918321	44.613697
3504.849982	994880.043501	44.618701
3504.866446	994798.883203	44.623706
3504.692628	994711.420111	44.628711
3504.734896	994613.397426	44.633716
3504.917038	994509.114246	44.638721
3504.773594	994446.585087	44.643725
3504.945673	994355.259572	44.648730
3504.750901	994272.080366	44.653735
3504.401017	994194.382088	44.658740
3504.721614	994108.874504	44.663745
3504.310294	994047.749239	44.668749
3504.163744	993960.172635	44.673754
3504.402632	993874.869871	44.678759
3504.041142	993802.332706	44.683764
3504.337703	993727.737285	44.688769
3504.133205	993654.392794	44.693773
3503.937452	993562.238069	44.698778
3504.111778	993504.128893	44.703783
3503.824866	993447.751775	44.708788
3504.427849	993365.012595	44.713793
3504.026320	993295.594058	44.718797
3504.549468	993222.319050	44.723802
3504.379089	993147.305636	44.728807
3504.195798	993070.928937	44.733812
3504.180773	993000.858385	44.738817
3504.263670	992941.004233	44.743821
3504.574299	992858.500757	44.748826
3504.020882	992790.660454	44.753831
3504.177732	992717.829128	44.758836
3504.306787	992645.586242	44.763841
3504.061939	992572.234415	44.768845
3503.920608	992495.063323	44.773850
3504.441636	992419.439076	44.778855
3504.252294	992354.847569	44.783860
3504.230650	992274.534701	44.788865
3504.008296	992211.896449	44.793869
3503.979969	992143.669507	44.798874
3504.157488	992072.873476	44.803879
3504.024086	992006.904139	44.808884
3504.382331	991928.765782	44.813889
3504.160121	991868.853111	44.818893
3504.018870	991799.080964	44.823898
3504.210912	991727.205952	44.828903
3504.112615	991652.843297	44.833908
3504.474006	991578.111506	44.838913
3504.109666	991510.224754	44.843917
3504.317425	991423.038092	44.848922
3504.066572	991350.938809	44.853927
3503.832737	991286.732436	44.858932
3504.351740	991209.922576	44.863937
3504.205851	991149.794770	44.868941
3504.125966	991079.906194	44.873946
3503.980810	991008.857581	44.878951
3504.197943	990932.971147	44.883956
3504.218372	990856.921105	44.888961
3504.019050	990808.108071	44.893965
3504.186068	990737.199643	44.898970
3504.132455	990657.259180	44.903975
3504.392322	990591.501140	44.908980
3504.508361	990514.455760	44.913985
3504.444801	990445.336715	44.918989
3504.149932	990374.207324	44.923994
3503.976865	990294.768964	44.928999
3504.318827	990227.238082	44.934004
3504.332932	990149.326980	44.939009
3504.264324	990085.567366	44.944013
3503.978845	990013.944372	44.949018
3504.178528	989949.456467	44.954023
3503.800371	989876.676862	44.959028
3503.967377	989806.439428	44.964033
3503.826971	989754.682205	44.969037
3504.062493	989681.994065	44.974042
3503.980568	989622.717221	44.979047
3504.291153	989549.429919	44.984052
3504.020739	989465.120053	44.989057
3503.940307	989400.964630	44.994061
3503.882829	989339.632857	44.999066
3504.026622	989270.562904	45.004071
3503.673249	989209.278460	45.009076
3504.325794	989148.217782	45.014081
3503.963020	989089.079158	45.019085
3504.083529	989014.743485	45.024090
3504.168418	988955.139626	45.029095
3503.796181	988887.125302	45.034100
3503.897342	988821.177887	45.039105
3504.065993	988749.756766	45.044109
3504.103066	988692.303748	45.049114
3504.070358	988610.770541	45.054119
3503.982142	988540.754596	45.059124
3504.037246	988462.521033	45.064129
3503.736382	988404.730621	45.069133
3503.955428	988338.368043	45.074138
3503.753658	988277.243663	45.079143
3503.728419	988212.187878	45.084148
3503.542999	988141.987952	45.089153
3503.436136	988088.454267	45.094157
3503.516816	988032.938291	45.099162
3503.379637	987975.311645	45.104167
3503.429209	987923.116283	45.109172
3503.664810	987850.307198	45.114177
3503.506437	987804.192971	45.119181
3503.492242	987742.349109	45.124186
3503.728034	987685.926255	45.129191
3503.327899	987622.583842	45.134196
3503.722182	987563.402215	45.139201
3503.624055	987519.519477	45.144205
3503.679089	987455.124697	45.149210
3504.009657	987376.733292	45.154215
3503.702608	987318.835310	45.159220
3503.874490	987266.711345	45.164225
3503.542638	987207.157824	45.169229
3503.616160	987139.927222	45.174234
3503.943812	987084.263763	45.179239
3503.705060	987035.034584	45.184244
3503.873215	986971.884016	45.189249
3503.503366	986908.431102	45.194253
3503.667024	986842.938304	45.199258
3503.482762	986785.697632	45.204263
3503.418039	986732.729655	45.209268
3503.562690	986656.798148	45.214273
3503.604384	986602.152765	45.219277
3503.843752	986548.157293	45.224282
3503.960389	986483.936529	45.229287
3503.491235	986423.811997	45.234292
3503.930933	986358.268166	45.239297
3503.678657	986309.913106	45.244301
3503.414258	986250.826341	45.249306
3503.800051	986174.751121	45.254311
3503.501714	986130.793078	45.259316
3503.964435	986075.487836	45.264321
3503.800422	986005.550774	45.269325
3503.846460	985939.091166	45.274330
3503.834328	985883.276786	45.279335
3503.732133	985839.674517	45.284340
3504.048416	985764.288348	45.289345
3503.750619	985701.200445	45.294349
3503.645856	985638.275221	45.299354
3503.626484	985579.043544	45.304359
3503.540787	985512.405484	45.309364
3503.795243	985450.590082	45.314369
3503.733195	985401.415262	45.319373
3503.457210	985341.247478	45.324378
3503.439576	985265.324164	45.329383
3503.438917	985231.362149	45.334388
3503.632793	985169.456084	45.339393
3503.558874	985112.765988	45.344397
3503.504041	985064.758215	45.349402
3503.562085	985004.629456	45.354407
3503.498301	984951.547168	45.359412
3503.813441	984893.912438	45.364417
3503.550764	984843.009068	45.369421
3503.332379	984780.581085	45.374426
3503.555464	984720.519749	45.379431
3503.224650	984662.013050	45.384436
3503.393510	984604.985110	45.389441
3503.198523	984562.364386	45.394445
3503.539121	984508.332929	45.399450
3503.741973	984450.809824	45.404455
3503.555735	984397.547333	45.409460
3503.645291	984323.350750	45.414465
3503.385173	984268.244658	45.419469
3503.413510	984209.966992	45.424474
3503.581667	984161.524444	45.429479
3503.573631	984120.431404	45.434484
3503.468737	984060.319526	45.439489
3503.177513	984016.051146	45.444493
3503.472529	983953.920006	45.449498
3503.521977	983896.026115	45.454503
3503.281956	983841.205431	45.459508
3503.613602	983780.140151	45.464513
3503.267736	983723.188174	45.469517
3503.781904	983669.705906	45.474522
3503.731120	983616.218567	45.479527
3503.588058	983564.893596	45.484532
3503.623171	983484.252049	45.489537
3503.689522	983440.310796	45.494541
3503.602025	983379.017388	45.499546
3503.384533	983322.430762	45.504551
3503.208907	983271.401390	45.509556
3503.645663	983211.288978	45.514561
3503.198277	983153.176497	45.519565
3503.651182	983108.485623	45.524570
3503.398389	983046.532463	45.529575
3503.018405	983002.368458	45.534580
3503.358429	982948.224702	45.539585
3503.449145	982903.006083	45.544589
3503.183153	982857.455321	45.549594
3503.429955	982799.713070	45.554599
3503.374885	982747.487540	45.559604
3503.499389	982685.077770	45.564609
3503.051057	982640.824584	45.569613
3502.925983	982590.366615	45.574618
3503.163318	982534.868921	45.579623
3503.414638	982486.300821	45.584628
3503.429382	982425.077965	45.589633
3503.107575	982376.798611	45.594637
3503.282983	982325.214748	45.599642
3503.132575	982275.539309	45.604647
3502.989851	982233.185493	45.609652
3503.229449	982168.700593	45.614657
3503.156318	982130.435655	45.619661
3503.259523	982096.047280	45.624666
3503.230404	982045.373395	45.629671
3503.268240	981997.226888	45.634676
3503.103718	981932.317638	45.639681
3503.058714	981888.382778	45.644685
3503.284405	981842.352327	45.649690
3503.211457	981784.847782	45.654695
3503.126911	981739.355857	45.659700
3503.298707	981683.763037	45.664705
3503.301370	981651.634579	45.669709
3503.041003	981600.506561	45.674714
3503.304825	981545.092545	45.679719
3502.971307	981482.842728	45.684724
3503.184416	981443.451812	45.689729
3502.958539	981400.226589	45.694733
3503.187577	981353.703359	45.699738
3503.108263	981295.706638	45.704743
3502.732639	981254.751162	45.709748
3503.014955	981213.491704	45.714753
3503.023265	981162.999146	45.719757
3502.918714	981116.431265	45.724762
3503.046579	981085.548624	45.729767
3502.849927	981050.031373	45.734772
3502.997555	980994.435826	45.739777
3503.015541	980953.804022	45.744781
3502.866359	980914.371464	45.749786
3503.271915	980875.042601	45.754791
3502.730405	980822.879579	45.759796
3503.016101	980770.286828	45.764801
3502.871707	980729.484835	45.769805
3502.646940	980680.003095	45.774810
3503.195253	980623.165893	45.779815
3502.881700	980504.838262	45.784820
3503.258872	980347.323963	45.789825
3503.074899	980135.001799	45.794829
3502.867421	979824.893372	45.799834
3502.876510	979483.862103	45.804839
3502.683189	979065.662633	45.809844
3502.730170	978593.654702	45.814849
3502.542241	978079.335966	45.819853
3502.386377	977461.181853	45.824858
3502.372255	976794.362430	45.829863
3502.044259	976068.867567	45.834868
3502.048027	975262.474164	45.839873
3502.017084	974394.568582	45.844877
3501.966124	973453.678596	45.849882
3501.974918	972443.178603	45.854887
3501.256537	971359.737471	45.859892
3501.420453	970189.741276	45.864897
3501.234550	968973.369475	45.869901
3500.925745	967653.875572	45.874906
3500.886928	966259.128299	45.879911
3500.828482	964794.409758	45.884916
3500.622185	963248.029758	45.889921
3500.068051	961611.430154	45.894925
3499.764751	959895.904795	45.899930
3500.002166	958102.610765	45.904935
3499.400851	956246.906948	45.909940
3499.409547	954296.708355	45.914945
3498.943361	952304.958630	45.919949
3498.275735	950255.235350	45.924954
3498.327083	948096.289908	45.929959
3497.508382	945880.932177	45.934964
3497.004610	943570.280440	45.939969
3496.888522	941197.275748	45.944973
3496.626751	938731.520925	45.949978
3496.500974	936190.501420	45.954983
3495.581345	933572.827639	45.959988
3495.316211	930871.333821	45.964993
3494.780109	928083.553565	45.969997
3494.142295	925222.410011	45.975002
3493.653961	922284.867232	45.980007
3493.277394	919259.746041	45.985012
3492.625634	916153.139069	45.990017
3492.140825	912983.542988	45.995021
3491.557256	909723.710791	46.000026
3491.214649	906379.615602	46.005031
3490.039009	902977.558361	46.010036
3489.806025	899479.574706	46.015041
3489.372189	895905.508457	46.020045
3488.399376	892233.620769	46.025050
3487.925305	888500.353025	46.030055
3486.897107	884699.773731	46.035060
3486.491209	880794.067968	46.040065
3486.009912	876823.897656	46.045069
3484.926349	872774.101893	46.050074
3484.324886	868639.410252	46.055079
3483.138036	864440.744469	46.060084
3482.732916	860142.079259	46.065089
3481.915543	855767.468424	46.070093
3480.882998	851333.694335	46.075098
3480.460060	846799.881876	46.080103
3479.312136	842195.084482	46.085108
3478.716790	837490.371301	46.090113
3477.833158	832721.301824	46.095117
3476.985002	827863.963369	46.100122
3476.355790	822934.456388	46.105127
3475.083630	817914.690327	46.110132
3474.220685	812818.096289	46.115137
3472.994913	807642.416876	46.120141
3472.275731	802379.574149	46.125146
3471.486274	797031.230791	46.130151
3470.179889	791617.461041	46.135156
3469.426617	786119.844329	46.140161
3468.069465	780537.005070	46.145165
3467.439891	774883.309442	46.150170
3466.311196	769121.935705	46.155175
3464.852486	763299.874202	46.160180
3463.780731	757378.126381	46.165185
3462.479290	751388.741211	46.170189
3461.539974	745331.383488	46.175194
3460.388431	739172.115378	46.180199
3459.224560	732940.600826	46.185204
3458.243255	726624.077921	46.190209
3456.969508	720237.087566	46.195213
3455.471475	713755.115487	46.200218
3454.522973	707193.893239	46.205223
3452.894141	700539.906622	46.210228
3451.410729	693818.367378	46.215233
3450.339663	687012.789355	46.220237
3449.200927	680119.917019	46.225242
3447.949145	673165.087490	46.230247
3446.181023	666123.279349	46.235252
3444.779288	658989.662384	46.240257
3443.343906	651795.637727	46.245261
3441.927586	644508.368278	46.250266
3440.667574	637154.663981	46.255271
3438.864313	629706.918658	46.260276
3437.814933	622191.045591	46.265281
3435.970677	614599.404382	46.270285
3434.684866	606930.132279	46.275290
3433.325265	599179.384379	46.280295
3430.982199	591348.582190	46.285300
3429.590068	583442.810775	46.290305
3427.871354	575465.540457	46.295309
3425.883132	567422.401678	46.300314
3424.407688	559278.019128	46.305319
3423.180977	551080.885957	46.310324
3421.123635	542809.090530	46.315329
3419.151837	534444.332330	46.320333
3417.404979	526011.021466	46.325338
3415.627878	517509.393598	46.330343
3413.445042	508941.580959	46.335348
3411.694951	500291.217464	46.340353
3409.714443	491581.222437	46.345357
3407.556349	482810.553848	46.350362
3405.847939	473949.561827	46.355367
3403.552979	465020.814414	46.360372
3401.670621	456031.485278	46.365377
3399.260242	446982.392122	46.370381
3397.022853	437861.252249	46.375386
3394.877105	428669.299660	46.380391
3392.686512	419434.902875	46.385396
3390.450597	410123.569462	46.390401
3388.113578	400737.970241	46.395405
3386.062514	391289.178343	46.400410
3383.819400	381797.608671	46.405415
3381.159640	372230.847403	46.410420
3378.700026	362611.891420	46.415425
3376.479738	352951.778641	46.420429
3373.551646	343211.009482	46.425434
3371.110576	333428.148976	46.430439
3368.307463	323607.234977	46.435444
3365.914530	313711.259862	46.440449
3363.092356	303779.347239	46.445453
3359.735296	293797.252426	46.450458
3357.036440	283748.327589	46.455463
3353.864480	273689.659114	46.460468
3350.671002	263583.166758	46.465473
3347.733586	253447.314805	46.470477
3344.421554	243253.683917	46.475482
3341.306098	233047.162278	46.480487
3337.831192	222743.359784	46.485492
3334.573137	212434.896854	46.490497
3331.096509	202126.009949	46.495501
3327.098639	191817.221262	46.500506
3323.282278	181468.894468	46.505511
3319.400722	171116.285871	46.510516
3315.902266	160743.139543	46.515521
3311.524918	150371.073630	46.520525
3307.058139	139986.771640	46.525530
3303.037649	129606.229041	46.530535
3297.626092	119248.607563	46.535540
3293.015315	108884.847178	46.540545
3287.416997	98538.864280	46.545549
3282.246961	88235.195423	46.550554
3276.754381	77971.966573	46.555559
3270.319098	67730.478234	46.560564
3263.509287	57565.353056	46.565569
3256.089775	47474.735674	46.570573
3247.784557	37474.965496	46.575578
3237.457899	27629.331354	46.580583
3215.620755	18244.509248	46.585588
3158.847608	10035.745694	46.590593
3091.624049	2779.035757	46.595597
2885.762756	362.797083	46.600602
2676.446615	361.106240	46.605607
2592.542023	357.561478	46.610612
2616.478811	337.989753	46.615617
2699.636825	318.423139	46.620621
2791.076179	315.647314	46.625626
2860.460794	308.979388	46.630631
2896.613616	307.927931	46.635636
2905.802486	319.745383	46.640641
2897.939567	306.585653	46.645645
2883.921322	294.803020	46.650650
2871.133540	291.276734	46.655655
2861.715560	297.000395	46.660660
2856.418560	301.405994	46.665665
2854.236485	304.331534	46.670669
2853.089350	304.740860	46.675674
2852.847423	281.689200	46.680679
2851.059284	278.022275	46.685684
2848.788114	284.154488	46.690689
2845.799465	291.533336	46.695693
2842.892771	286.545287	46.700698
2840.125991	282.546210	46.705703
2836.201381	279.751131	46.710708
2833.251287	273.180567	46.715713
2830.283236	273.750484	46.720717
2827.058183	288.328028	46.725722
2824.097435	273.266336	46.730727
2820.632894	288.568445	46.735732
2817.934475	275.985998	46.740737
2814.933333	264.370200	46.745741
2811.395268	272.619222	46.750746
2807.854658	271.184293	46.755751
2804.126586	269.234889	46.760756
2801.405432	261.250025	46.765761
2798.653664	254.083649	46.770765
2794.996829	264.460476	46.775770
2792.189510	260.254809	46.780775
2788.250739	264.320994	46.785780
2785.005012	259.493746	46.790785
2781.789261	263.070176	46.795789
2778.252219	270.041617	46.800794
2774.747611	250.211914	46.805799
2771.632640	258.180260	46.810804
2768.260645	268.460119	46.815809
2765.199867	247.400489	46.820813
2761.414694	251.888084	46.825818
2758.259647	245.580636	46.830823
2755.051028	253.151442	46.835828
2751.586315	245.106680	46.840833
2748.062277	257.403605	46.845837
2744.402829	257.285849	46.850842
2741.240352	245.452326	46.855847
2737.351760	250.874499	46.860852
2734.262406	251.299693	46.865857
2730.937043	254.245240	46.870861
2727.303095	251.045656	46.875866
2724.327432	245.498307	46.880871
2721.043131	252.061085	46.885876
2717.597445	242.898174	46.890881
2714.196884	250.665594	46.895885
2710.032837	251.976346	46.900890
2706.613934	245.217558	46.905895
2703.810191	248.750256	46.910900
2700.508613	242.423587	46.915905
2696.862818	235.328205	46.920909
2693.176410	246.704993	46.925914
2689.805190	235.337254	46.930919
2686.327649	242.187819	46.935924
2682.278399	236.973675	46.940929
2679.472075	228.243852	46.945933
2676.449346	230.713615	46.950938
2672.726103	231.479631	46.955943
2668.650758	236.547659	46.960948
2665.278916	224.993285	46.965953
2661.902382	233.782399	46.970957
2658.502195	244.912225	46.975962
2655.747577	229.594997	46.980967
2651.745840	242.609710	46.985972
2648.502839	231.635810	46.990977
2645.405018	231.485287	46.995981
2641.569020	244.851326	47.000986
2637.984782	231.687950	47.005991
2634.605968	238.007657	47.010996
2631.206649	249.368605	47.016001
2628.017112	226.052905	47.021005
2623.502637	235.390943	47.026010
2620.581365	232.449301	47.031015
2616.992710	231.606442	47.036020
2613.885768	234.369019	47.041025
2610.516964	234.115302	47.046029
2606.777900	236.952907	47.051034
2603.468572	229.662795	47.056039
2599.777371	233.505526	47.061044
2596.407655	219.601610	47.066049
2593.397697	222.067225	47.071053
2589.831847	225.235092	47.076058
2586.159424	215.461673	47.081063
2582.065501	221.143095	47.086068
2578.887030	225.048093	47.091073
2575.203911	220.608781	47.096077
2571.799352	229.749918	47.101082
2568.789308	233.825550	47.106087
2565.130952	229.543364	47.111092
2561.540772	224.645169	47.116097
2558.047380	225.555855	47.121101
2554.664809	223.331580	47.126106
2550.977431	214.704581	47.131111
2547.194007	228.309207	47.136116
2544.466485	222.460475	47.141121
2541.031468	207.638116	47.146125
2537.360394	224.002703	47.151130
2533.961453	216.898679	47.156135
2530.087391	218.442091	47.161140
2526.722028	225.110342	47.166145
2523.462505	218.239449	47.171149
2519.496154	214.017353	47.176154
2516.406990	211.463641	47.181159
2512.953356	218.972015	47.186164
2509.515545	215.652500	47.191169
2506.004916	218.998054	47.196173
2502.297542	222.077911	47.201178
2498.946340	210.303291	47.206183
2495.592665	217.119286	47.211188
2491.803673	212.616580	47.216193
2488.251211	213.539701	47.221197
2484.911198	213.395835	47.226202
2481.673216	202.289512	47.231207
2478.135732	215.982737	47.236212
2474.664248	212.685959	47.241217
2470.919508	216.493077	47.246221
2467.227046	201.258412	47.251226
2463.729383	206.484817	47.256231
2460.480257	217.188834	47.261236
2456.975073	209.930019	47.266241
2453.462595	203.692135	47.271245
2449.900005	216.348182	47.276250
2446.666765	208.526973	47.281255
2443.087866	212.132328	47.286260
2439.820736	225.206411	47.291265
2436.367301	211.264805	47.296269
2432.207486	207.331271	47.301274
2428.998411	200.385718	47.306279
2425.867345	211.209873	47.311284
2421.944672	206.695709	47.316289
2418.877229	198.026843	47.321293
2415.186468	203.226606	47.326298
2411.804456	200.286551	47.331303
2407.951460	201.154298	47.336308
2404.783347	194.504093	47.341313
2401.562924	201.650643	47.346317
2397.736470	198.670631	47.351322
2394.372698	194.896786	47.356327
2390.635951	203.904713	47.361332
2387.021753	203.783908	47.366337
2383.912927	205.695762	47.371341
2380.171297	209.372574	47.376346
2376.918955	190.907281	47.381351
2373.214199	203.565479	47.386356
2369.539330	201.020225	47.391361
2366.125400	188.061700	47.396365
2362.368287	199.853643	47.401370
2359.519700	196.955476	47.406375
2355.723489	204.927359	47.411380
2352.174419	190.242528	47.416385
2348.794150	193.336084	47.421389
2344.473464	196.248215	47.426394
2341.571933	190.393947	47.431399
2338.238163	201.315481	47.436404
2335.049884	197.029401	47.441409
2331.602271	192.562931	47.446413
2327.852079	198.876405	47.451418
2324.647085	199.126182	47.456423
2321.302281	184.215307	47.461428
2317.440757	187.846210	47.466433
2313.898183	194.212957	47.471437
2310.049471	194.855108	47.476442
2306.878377	191.571228	47.481447
2303.216138	193.145324	47.486452
2299.908049	188.935948	47.491457
2296.659304	184.939554	47.496461
2293.106987	187.875145	47.501466
2289.238339	182.203491	47.506471
2285.616010	185.121429	47.511476
2282.072605	189.686157	47.516481
2278.816172	184.527874	47.521485
2275.394328	197.065943	47.526490
2271.772679	191.098037	47.531495
2268.211812	188.675115	47.536500
2264.867380	185.250055	47.541505
2261.441030	181.359629	47.546509
2258.226480	190.758382	47.551514
2254.665697	183.981230	47.556519
2250.892139	184.304488	47.561524
2247.113271	194.649506	47.566529
2243.871177	186.087085	47.571533
2239.856918	193.486951	47.576538
2236.666640	183.666203	47.581543
2233.286708	188.500058	47.586548
2229.742248	194.214534	47.591553
2226.692211	185.206875	47.596557
2223.189838	187.400647	47.601562
2219.388077	187.139098	47.606567
2215.399482	173.038793	47.611572
2212.153561	188.589252	47.616577
2209.108652	174.837241	47.621581
2205.526910	177.597476	47.626586
2202.149862	174.297106	47.631591
2198.630392	180.914617	47.636596
2195.067673	177.167966	47.641601
2191.166936	175.513939	47.646605
2188.058909	181.681001	47.651610
2184.546063	182.951017	47.656615
2180.656320	183.257760	47.661620
2177.182338	186.624536	47.666625
2173.827204	178.974533	47.671629
2170.324075	185.021493	47.676634
2167.032961	175.391845	47.681639
2163.450589	181.216976	47.686644
2159.702488	186.043514	47.691649
2156.511961	182.717133	47.696653
2152.859288	183.949553	47.701658
2149.149451	183.874434	47.706663
2145.536052	181.400948	47.711668
2142.088290	177.742208	47.716673
2139.458915	178.137052	47.721677
2135.560658	181.964211	47.726682
2131.883260	176.136304	47.731687
2128.738898	185.290986	47.736692
2125.151371	185.878705	47.741697
2121.526774	171.913174	47.746701
2117.708006	189.304668	47.751706
2114.358318	172.514436	47.756711
2110.725221	172.837879	47.761716
2107.216624	175.976971	47.766721
2104.061373	173.016735	47.771725
2100.356061	185.146505	47.776730
2096.904401	178.184318	47.781735
2093.183222	169.072174	47.786740
2090.138886	175.916794	47.791745
2086.574963	172.559206	47.796749
2083.072720	170.277261	47.801754
2079.527380	176.819470	47.806759
2075.657856	166.180333	47.811764
2072.125061	169.455631	47.816769
2068.952035	173.382307	47.821773
2065.533470	181.006297	47.826778
2061.692298	163.069992	47.831783
2058.385015	175.223397	47.836788
2054.627997	181.267593	47.841793
2051.449535	170.794066	47.846797
2047.539348	181.087712	47.851802
2044.759557	175.324787	47.856807
2041.062722	173.966126	47.861812
2037.424372	175.922154	47.866817
2034.163315	173.390210	47.871821
2030.265697	173.354316	47.876826
2026.891285	170.500018	47.881831
2023.234297	178.394802	47.886836
2019.700881	171.061386	47.891841
2016.333291	170.935007	47.896845
2012.929628	178.341486	47.901850
2009.869568	172.187170	47.906855
2006.124011	179.043610	47.911860
2002.223752	179.818433	47.916865
1999.193706	177.608690	47.921869
1994.856682	183.855932	47.926874
1991.543037	167.752900	47.931879
1988.401939	166.368888	47.936884
1984.545933	168.639748	47.941889
1981.480010	165.329303	47.946893
1978.068059	169.365869	47.951898
1974.597539	166.450599	47.956903
1970.953480	171.389296	47.961908
1967.373617	177.822213	47.966913
1963.885026	173.411533	47.971917
1960.238400	176.415412	47.976922
1957.032289	173.024218	47.981927
1953.536626	167.541822	47.986932
1949.663371	171.141883	47.991937
1946.824856	163.795884	47.996941
1942.902368	170.074109	48.001946
1939.360386	171.531756	48.006951
1935.562790	167.178482	48.011956
1932.225332	172.159648	48.016961
1928.888007	167.735181	48.021965
1924.832214	168.356741	48.026970
1921.992756	154.127556	48.031975
1918.072388	159.928928	48.036980
1914.915373	165.800992	48.041985
1911.489060	156.423572	48.046989
1907.972457	167.932502	48.051994
1904.575050	156.950603	48.056999
1901.107168	161.154968	48.062004
1897.545655	161.623570	48.067009
1893.972640	156.857491	48.072013
1890.132799	169.406812	48.077018
1887.099318	160.231854	48.082023
1883.311734	163.785355	48.087028
1879.471334	161.600738	48.092033
1876.486784	159.586778	48.097037
1872.751144	163.454419	48.102042
1869.426870	155.566277	48.107047
1865.917014	154.871403	48.112052
1861.913710	155.527746	48.117057
1859.163250	149.653328	48.122061
1855.231752	156.765537	48.127066
1851.989778	151.140225	48.132071
1848.362663	148.377337	48.137076
1844.808464	157.801268	48.142081
1841.614193	156.266766	48.147085
1837.626612	148.881523	48.152090
1834.099723	155.868977	48.157095
1830.902374	153.885608	48.162100
1826.982544	154.447399	48.167105
1824.095024	162.242238	48.172109
1820.366618	155.563240	48.177114
1816.657223	151.066149	48.182119
1813.257475	149.433757	48.187124
1809.472299	157.589109	48.192129
1806.516515	142.568532	48.197133
1802.888609	167.991788	48.202138
1799.273554	164.431072	48.207143
1795.878064	152.601565	48.212148
1792.100512	158.882482	48.217153
1789.192015	148.635088	48.222157
1785.347702	152.614718	48.227162
1781.903706	154.229314	48.232167
1778.287470	146.926779	48.237172
1774.636648	156.303539	48.242177
1771.486631	149.391122	48.247181
1767.830312	158.904544	48.252186
1764.110994	150.590828	48.257191
1760.535076	146.846790	48.262196
1757.104034	145.686628	48.267201
1753.782202	138.688034	48.272205
1750.045544	162.463330	48.277210
1747.195908	150.513501	48.282215
1743.293404	149.256219	48.287220
1739.160628	150.919666	48.292225
1736.434876	148.938144	48.297229
1732.588441	161.076917	48.302234
1729.749863	156.183924	48.307239
1726.146758	150.369748	48.312244
1722.228325	146.153548	48.317249
1718.956217	147.192664	48.322253
1714.925530	146.863198	48.327258
1711.581471	151.544636	48.332263
1708.109971	148.308049	48.337268
1704.716150	161.732421	48.342273
1701.440917	146.546877	48.347277
1697.570342	153.245307	48.352282
1694.171859	146.576963	48.357287
1691.065829	152.128150	48.362292
1687.023517	159.552424	48.367297
1683.847035	153.536071	48.372301
1680.100005	160.022535	48.377306
1676.460470	153.818392	48.382311
1673.378963	141.633494	48.387316
1670.237807	154.214993	48.392321
1666.319359	149.159264	48.397325
1662.634618	163.388052	48.402330
1658.968594	154.814524	48.407335
1655.753370	146.468010	48.412340
1652.284030	143.458500	48.417345
1648.855437	154.335503	48.422349
1644.854986	152.463335	48.427354
1641.625157	139.511118	48.432359
1638.008120	148.938293	48.437364
1634.620162	145.205630	48.442369
1631.390268	141.924777	48.447373
1627.341376	158.016305	48.452378
1624.288068	136.894763	48.457383
1620.838893	143.324895	48.462388
1616.964050	145.668996	48.467393
1613.807902	144.875628	48.472397
1610.304607	161.887470	48.477402
1606.885110	148.033278	48.482407
1603.173367	141.980400	48.487412
1599.686176	149.602267	48.492417
1596.217362	142.630182	48.497421
1592.670639	145.285965	48.502426
1589.033449	144.885025	48.507431
1585.672004	142.126582	48.512436
1581.897691	137.804801	48.517441
1578.552482	148.918652	48.522445
1574.897074	147.873839	48.527450
1571.661418	148.573845	48.532455
1568.256995	146.048128	48.537460
1564.658545	148.399130	48.542465
1561.591222	139.222048	48.547469
1557.203555	157.051493	48.552474
1554.383679	139.165470	48.557479
1550.838445	138.178454	48.562484
1547.075526	154.421116	48.567489
1543.349811	136.426900	48.572493
1540.117302	130.789145	48.577498
1536.604463	144.239711	48.582503
1533.146224	139.858890	48.587508
1529.627442	143.084268	48.592513
1526.489843	140.730301	48.597517
1522.534904	144.118425	48.602522
1518.777907	146.507452	48.607527
1515.146820	141.877252	48.612532
1512.009257	140.128638	48.617537
1508.960376	138.300671	48.622541
1505.284795	147.162398	48.627546
1501.829173	135.284503	48.632551
1498.264855	148.639894	48.637556
1494.163080	148.528180	48.642561
1490.932066	138.767175	48.647565
1487.539440	142.140947	48.652570
1484.315512	150.119464	48.657575
1480.251016	143.580294	48.662580
1476.715676	136.804337	48.667585
1473.588678	142.525397	48.672589
1469.928061	152.287767	48.677594
1466.805114	144.691599	48.682599
1463.324102	143.217028	48.687604
1459.670015	146.501766	48.692609
1456.575894	139.064716	48.697613
1452.365519	142.350404	48.702618
1449.070157	144.610300	48.707623
1445.614937	135.885216	48.712628
1441.756671	149.044968	48.717633
1438.521513	137.912671	48.722637
1434.705755	140.290819	48.727642
1431.499015	146.817658	48.732647
1428.092245	132.646881	48.737652
1424.398061	129.781149	48.742657
1421.223436	128.140311	48.747661
1417.707876	135.046151	48.752666
1414.148960	137.799430	48.757671
1410.544027	139.668458	48.762676
1406.583499	138.107120	48.767681
1403.364893	137.863015	48.772685
1400.127832	130.694947	48.777690
1396.373343	134.775369	48.782695
1393.459702	134.683672	48.787700
1389.434027	145.294681	48.792705
1386.258714	133.015237	48.797709
1382.479076	142.681559	48.802714
1378.879046	139.850822	48.807719
1375.356330	131.170366	48.812724
1371.777501	144.691569	48.817729
1368.674684	146.264253	48.822733
1364.958158	142.353036	48.827738
1361.456005	139.907881	48.832743
1357.751989	135.111144	48.837748
1354.211463	135.512229	48.842753
1350.892230	122.875955	48.847757
1347.310837	133.925174	48.852762
1343.962566	135.593431	48.857767
1340.622696	134.493506	48.862772
1337.064405	135.899281	48.867777
1333.658055	135.556464	48.872781
1329.818266	143.342693	48.877786
1326.461911	130.686708	48.882791
1322.844613	142.825305	48.887796
1319.115091	140.424409	48.892801
1315.934638	122.185980	48.897805
1312.171550	134.133076	48.902810
1308.878394	136.156094	48.907815
1305.566445	137.266889	48.912820
1302.057658	139.532580	48.917825
1298.520721	130.112332	48.922829
1295.100231	132.487067	48.927834
1291.518503	131.385850	48.932839
1288.199522	130.992231	48.937844
1284.173021	127.645043	48.942849
1280.980284	131.372937	48.947853
1277.126164	130.563033	48.952858
1273.695916	131.509179	48.957863
1270.204494	125.475485	48.962868
1266.776331	134.091757	48.967873
1263.349953	113.852783	48.972877
1259.767643	130.371939	48.977882
1256.035965	126.455596	48.982887
1253.064426	126.299622	48.987892
1249.573124	131.642476	48.992897
1246.197412	128.931453	48.997901
1242.305126	135.794091	49.002906
1238.932141	138.979655	49.007911
1235.368917	140.357092	49.012916
1231.941512	130.153238	49.017921
1228.274154	125.777707	49.022925
1224.377608	128.976597	49.027930
1221.220884	136.661860	49.032935
1217.888627	127.679252	49.037940
1214.434712	126.352958	49.042945
1210.942457	124.213761	49.047949
1207.201870	129.780691	49.052954
1203.597108	128.885863	49.057959
1200.413387	133.999893	49.062964
1196.678639	128.959023	49.067969
1193.315557	130.752720	49.072973
1189.982793	134.594532	49.077978
1186.332243	137.362061	49.082983
1182.818095	128.259148	49.087988
1179.279060	145.458634	49.092993
1175.822651	129.079131	49.097997
1172.237880	121.466042	49.103002
1168.533766	138.902517	49.108007
1165.339527	132.407638	49.113012
1161.826219	141.728896	49.118017
1158.378537	130.181688	49.123021
1154.720803	136.923568	49.128026
1151.161600	129.997150	49.133031
1147.727441	130.378017	49.138036
1144.161037	130.309047	49.143041
1140.648566	130.219928	49.148045
1137.155612	125.609766	49.153050
1133.899073	135.587715	49.158055
1130.763195	122.548292	49.163060
1126.809177	129.948193	49.168065
1123.661130	126.765664	49.173069
1119.760648	127.225108	49.178074
1116.077299	131.656187	49.183079
1112.462231	133.630526	49.188084
1108.704217	130.019614	49.193089
1105.674181	133.866931	49.198093
1102.385385	142.584078	49.203098
1098.856622	122.330050	49.208103
1095.424881	127.891724	49.213108
1091.602423	130.764730	49.218113
1088.434045	128.035443	49.223117
1084.615836	131.052085	49.228122
1081.244081	134.297795	49.233127
1077.867489	130.489661	49.238132
1074.272737	139.451187	49.243137
1070.770802	124.597780	49.248141
1066.974612	127.800805	49.253146
1063.477238	144.700149	49.258151
1060.133078	129.339061	49.263156
1056.532502	128.605909	49.268161
1053.611627	126.594141	49.273165
1049.726595	129.608613	49.278170
1045.738614	122.827733	49.283175
1042.566298	120.144601	49.288180
1038.685303	138.719110	49.293185
1036.043407	125.461055	49.298189
1032.112988	124.085769	49.303194
1028.604182	124.681263	49.308199
1025.039129	136.063442	49.313204
1021.866099	130.356948	49.318209
1018.561573	124.078362	49.323213
1014.968768	131.660091	49.328218
1011.410735	127.754192	49.333223
1007.819571	115.459295	49.338228
1003.968624	129.770891	49.343233
1000.480419	128.777510	49.348237
997.263734	124.516533	49.353242
993.199045	130.103339	49.358247
990.046690	120.303897	49.363252
986.355966	117.055952	49.368257
983.294561	127.527764	49.373261
979.613928	120.860050	49.378266
976.297677	118.906790	49.383271
972.882257	126.224548	49.388276
968.941135	128.230499	49.393281
965.524469	129.128877	49.398285
962.088506	125.765087	49.403290
958.714669	127.402329	49.408295
955.548956	117.390441	49.413300
951.378460	134.028133	49.418305
948.079870	121.307213	49.423309
944.130770	124.742331	49.428314
941.022187	116.975584	49.433319
937.546163	120.619187	49.438324
933.814648	118.061885	49.443329
930.538002	120.168080	49.448333
927.141210	118.355903	49.453338
923.427569	120.794114	49.458343
920.210651	123.262777	49.463348
916.591938	122.725171	49.468353
913.365577	121.608594	49.473357
909.784286	128.467497	49.478362
906.197759	124.164146	49.483367
902.511995	120.305643	49.488372
898.653453	131.179620	49.493377
895.499209	125.990104	49.498381
891.823427	123.415335	49.503386
888.157638	122.528486	49.508391
885.239397	115.982768	49.513396
881.451563	122.253470	49.518401
878.077558	114.338999	49.523405
874.600266	130.452148	49.528410
871.087087	125.360784	49.533415
867.807476	120.783422	49.538420
864.130820	135.429450	49.543425
860.554855	116.205173	49.548429
856.870860	123.079380	49.553434
853.240761	121.832880	49.558439
850.309221	119.443934	49.563444
846.305541	114.089968	49.568449
842.908180	121.535318	49.573453
839.441755	125.924991	49.578458
835.878238	116.875537	49.583463
832.387853	122.433297	49.588468
828.766528	119.902847	49.593473
825.712540	120.204427	49.598477
821.931743	116.136930	49.603482
818.250731	113.447939	49.608487
815.010667	110.194737	49.613492
811.235285	119.957281	49.618497
808.682985	110.224800	49.623501
804.656252	117.541664	49.628506
800.912193	118.888314	49.633511
797.389795	110.074395	49.638516
793.484055	121.651824	49.643521
790.355711	116.048277	49.648525
787.029842	117.022809	49.653530
783.438250	119.035072	49.658535
780.061842	115.518303	49.663540
776.215892	112.566332	49.668545
772.952445	115.241337	49.673549
769.314516	122.696356	49.678554
765.713131	121.787397	49.683559
762.321472	113.792645	49.688564
759.048813	119.734161	49.693569
755.508832	106.075175	49.698573
752.123240	122.746400	49.703578
748.524957	117.189800	49.708583
745.181643	115.767650	49.713588
741.228032	122.471765	49.718593
737.828071	110.269783	49.723597
734.344509	114.212960	49.728602
730.692814	115.317193	49.733607
727.246101	112.128746	49.738612
723.630025	112.950768	49.743617
720.475216	115.776063	49.748621
716.974900	119.776967	49.753626
713.358419	114.148614	49.758631
709.829899	110.529346	49.763636
706.501456	129.110089	49.768641
703.268163	115.508903	49.773645
699.412557	118.497987	49.778650
695.766494	114.417097	49.783655
692.337175	118.660226	49.788660
688.519822	119.432539	49.793665
685.140261	112.705820	49.798669
681.847324	110.940155	49.803674
678.218041	117.781930	49.808679
675.174074	106.380680	49.813684
671.420943	123.566740	49.818689
667.676785	114.598726	49.823693
664.166865	119.179852	49.828698
660.579185	123.724792	49.833703
657.335073	113.198522	49.838708
653.974049	113.801669	49.843713
650.391916	112.986474	49.848717
646.745265	113.750942	49.853722
642.922336	114.688463	49.858727
639.857878	107.503174	49.863732
636.184486	113.974899	49.868737
632.810052	105.664550	49.873741
629.608099	101.843906	49.878746
625.804849	107.711511	49.883751
622.301115	110.608486	49.888756
618.484866	114.910325	49.893761
614.924612	117.185348	49.898765
611.810011	104.412071	49.903770
608.111930	108.750236	49.908775
604.952958	113.332816	49.913780
601.004783	120.600805	49.918785
597.762447	111.788109	49.923789
594.644457	116.326733	49.928794
590.889189	111.766230	49.933799
587.614942	105.227576	49.938804
583.542981	126.106886	49.943809
580.099661	106.608268	49.948813
576.744231	102.268526	49.953818
573.299705	109.345509	49.958823
570.090907	111.936012	49.963828
566.118056	116.721898	49.968833
562.899912	105.923948	49.973837
559.059960	121.157908	49.978842
555.570898	119.893706	49.983847
552.346996	106.407486	49.988852
548.544954	117.162481	49.993857
545.365420	113.794453	49.998861
541.743546	107.925691	50.003866
537.918030	104.878546	50.008871
534.591532	111.981434	50.013876
531.087843	124.320686	50.018881
527.848148	102.736460	50.023885
524.219326	111.475949	50.028890
520.308878	119.993326	50.033895
517.171313	107.217090	50.038900
513.633102	110.334882	50.043905
510.147178	103.450923	50.048909
506.399550	111.083805	50.053914
503.112574	107.480203	50.058919
499.469402	112.766502	50.063924
495.906628	102.018122	50.068929
492.890755	98.734572	50.073933
490.022538	110.065779	50.078938
485.868312	107.199734	50.083943
482.503203	103.766700	50.088948
478.467048	108.092014	50.093953
475.138142	109.822895	50.098957
471.339027	105.708330	50.103962
467.426071	100.586863	50.108967
464.774153	103.524932	50.113972
461.060756	103.735039	50.118977
457.875290	99.436348	50.123981
454.034944	113.321606	50.128986
450.568605	108.233412	50.133991
447.298914	99.758191	50.138996
443.468199	109.022168	50.144001
439.858501	98.344324	50.149005
436.880650	102.882356	50.154010
433.200611	113.399519	50.159015
429.848508	108.317328	50.164020
425.752578	112.748341	50.169025
422.466201	102.377876	50.174029
419.120836	104.870847	50.179034
415.404089	110.196274	50.184039
412.025902	101.885399	50.189044
408.393964	97.534408	50.194049
404.882868	96.259331	50.199053
401.813920	101.435823	50.204058
397.872354	100.859006	50.209063
394.747195	94.441354	50.214068
391.002911	101.100215	50.219073
387.601437	95.626362	50.224077
384.245528	101.175233	50.229082
380.933735	105.994866	50.234087
377.277906	87.557535	50.239092
373.466081	103.710117	50.244097
369.741730	98.968355	50.249101
366.470824	97.215595	50.254106
362.830479	95.194757	50.259111
359.898356	96.379108	50.264116
356.179870	95.209350	50.269121
352.384215	96.858664	50.274125
348.747228	95.486425	50.279130
345.256092	84.389420	50.284135
341.931590	99.664181	50.289140
338.407365	109.755502	50.294145
335.142702	83.421811	50.299149
331.265308	98.929188	50.304154
327.868739	108.312000	50.309159
324.717942	94.126338	50.314164
320.916895	103.229498	50.319169
317.552199	101.467891	50.324173
313.713159	96.458619	50.329178
310.146361	104.495109	50.334183
307.523644	101.914624	50.339188
303.257076	111.736945	50.344193
300.116036	102.191170	50.349197
296.187450	95.553025	50.354202
292.623816	91.337325	50.359207
289.270561	97.581608	50.364212
285.716346	107.976631	50.369217
282.700699	99.174131	50.374221
279.393010	91.276896	50.379226
275.747173	104.368086	50.384231
272.164017	96.263216	50.389236
268.121222	107.513304	50.394241
264.519021	103.046106	50.399245
261.091957	102.177690	50.404250
257.670617	96.583878	50.409255
254.576915	94.232271	50.414260
250.853606	113.099164	50.419265
247.525386	99.614103	50.424269
243.966733	99.625730	50.429274
240.262750	98.203950	50.434279
237.123428	102.209373	50.439284
233.121679	105.343912	50.444289
229.719906	87.116189	50.449293
226.498514	106.100522	50.454298
223.091863	97.705187	50.459303
219.827383	91.233801	50.464308
216.161575	105.916254	50.469313
212.192512	103.967869	50.474317
208.875974	97.932063	50.479322
205.334880	95.921557	50.484327
202.038766	86.512557	50.489332
198.191207	94.157754	50.494337
195.094167	96.246659	50.499341
191.581501	91.289894	50.504346
187.556061	103.598770	50.509351
184.192390	90.634691	50.514356
180.498417	95.526045	50.519361
177.080091	92.281628	50.524365
173.900264	96.832422	50.529370
170.255212	101.233873	50.534375
167.255448	99.129801	50.539380
163.669447	100.370387	50.544385
159.907112	99.412008	50.549389
156.275777	105.404564	50.554394
152.573410	98.643704	50.559399
149.514531	89.926070	50.564404
145.681922	109.507062	50.569409
142.338082	99.425066	50.574413
138.771590	103.740353	50.579418
135.008998	102.080008	50.584423
131.664033	99.781128	50.589428
128.340455	107.253959	50.594433
125.031559	105.859601	50.599437
121.436795	93.719625	50.604442
117.775745	97.655141	50.609447
114.866669	92.806056	50.614452
110.626264	99.826032	50.619457
107.177403	87.051787	50.624461
103.733792	92.183173	50.629466
100.188153	97.315538	50.634471
96.768551	89.158999	50.639476
93.252266	92.265588	50.644481
89.637594	93.708853	50.649485
86.080607	95.203260	50.654490
82.378302	101.211230	50.659495
79.270921	99.267736	50.664500
75.706280	98.291637	50.669505
72.162493	90.942498	50.674509
68.685881	95.324356	50.679514
65.430579	105.484514	50.684519
62.495356	88.984692	50.689524
58.111381	94.798009	50.694529
54.400520	94.216630	50.699533
51.057642	91.147852	50.704538
47.478451	98.878612	50.709543
44.420843	95.409910	50.714548
40.665272	95.058391	50.719553
37.119942	95.789487	50.724557
33.838889	87.990305	50.729562
29.947770	97.483082	50.734567
27.039234	95.846915	50.739572
22.961654	92.758193	50.744577
19.410437	95.773124	50.749581
16.336331	90.404228	50.754586
12.711576	102.719586	50.759591
9.691390	90.503780	50.764596
5.473544	103.593918	50.769601
2.112665	92.003059	50.774605