Thu Jun 16 11:22:48 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.780399	97.154583	0.000000
0.636628	98.542729	0.005005
0.871811	97.729240	0.010010
0.664208	88.408620	0.015014
0.222894	87.265157	0.020019
0.339909	80.697001	0.025024
0.110506	59.328285	0.030029
-0.419134	56.456510	0.035034
-0.922786	56.411795	0.040038
-1.192377	44.463749	0.045043
-1.249071	40.844654	0.050048
-1.390281	35.157843	0.055053
-1.725461	32.109312	0.060058
-2.018263	25.599039	0.065062
-2.515267	28.277042	0.070067
-2.787151	10.855133	0.075072
-2.875835	13.185480	0.080077
-3.595832	18.364591	0.085082
-3.718225	11.345426	0.090086
-3.788989	21.054142	0.095091
-4.721786	8.817265	0.100096
-5.383052	10.062147	0.105101
-4.593194	22.109470	0.110106
-4.958404	4.786254	0.115110
-5.634013	6.664590	0.120115
-5.148290	4.121353	0.125120
-5.481657	12.404023	0.130125
-5.615149	6.538767	0.135130
-5.634888	8.313352	0.140134
-6.929925	19.670446	0.145139
-7.184128	8.078885	0.150144
-6.965587	19.355926	0.155149
-7.355579	25.522379	0.160154
-6.919003	12.396643	0.165158
-7.677973	23.901327	0.170163
-8.367518	16.218625	0.175168
-8.722278	24.636638	0.180173
-9.044150	22.865343	0.185178
-8.491927	17.697494	0.190182
-9.085654	19.255686	0.195187
-8.913053	13.816633	0.200192
-8.741787	12.638040	0.205197
-9.340922	19.514532	0.210202
-10.073499	10.227544	0.215206
-10.143504	22.945648	0.220211
-9.984500	11.891530	0.225216
-11.007260	15.488458	0.230221
-11.592370	11.357871	0.235226
-11.595322	16.151330	0.240230
-11.760273	14.799918	0.245235
-11.665415	5.346793	0.250240
-11.969163	18.323715	0.255245
-12.030504	10.243312	0.260250
-11.823799	11.630454	0.265254
-12.489191	19.807687	0.270259
-13.042306	1.414068	0.275264
-13.451912	14.621276	0.280269
-13.416692	21.360083	0.285274
-13.391418	16.634272	0.290278
-13.900684	25.155755	0.295283
-14.441859	24.802341	0.300288
-14.811755	18.448157	0.305293
-15.232644	24.461673	0.310298
-15.226297	14.205434	0.315302
-15.209565	28.496143	0.320307
-15.039224	20.078824	0.325312
-15.492704	19.848342	0.330317
-16.105193	27.492593	0.335322
-16.316334	19.729153	0.340326
-16.514908	29.368431	0.345331
-16.700141	15.597958	0.350336
-16.788649	17.992796	0.355341
-16.975058	31.579153	0.360346
-17.360835	20.204465	0.365350
-18.247897	16.787123	0.370355
-18.323298	20.104175	0.375360
-18.198949	22.226280	0.380365
-18.516252	13.559361	0.385370
-18.267181	23.311902	0.390374
-18.921898	25.583374	0.395379
-19.283655	19.698914	0.400384
-19.714645	18.656647	0.405389
-20.157703	21.515544	0.410394
-19.648025	11.063859	0.415398
-20.027590	27.369839	0.420403
-20.379051	18.037129	0.425408
-20.852716	20.920518	0.430413
-21.712869	21.514111	0.435418
-21.511637	13.593145	0.440422
-21.599884	21.669968	0.445427
-21.767516	16.405033	0.450432
-21.562581	18.857330	0.455437
-21.833923	17.285548	0.460442
-22.246804	14.387682	0.465446
-22.839707	28.196789	0.470451
-23.026955	19.408932	0.475456
-22.727783	21.649138	0.480461
-23.418689	14.524549	0.485466
-23.911418	26.485209	0.490470
-24.524155	28.478547	0.495475
-24.636117	13.030209	0.500480
-24.613507	26.404639	0.505485
-24.731002	19.020633	0.510490
-24.512901	12.068713	0.515494
-25.040934	24.141554	0.520499
-25.406562	18.708284	0.525504
-25.486336	4.039915	0.530509
-25.925865	14.681464	0.535514
-25.883244	14.677485	0.540518
-26.832633	24.568103	0.545523
-27.120556	23.197256	0.550528
-27.618878	24.149737	0.555533
-27.558289	16.099989	0.560538
-27.500366	20.401467	0.565542
-27.861788	22.988303	0.570547
-27.921980	12.218228	0.575552
-27.693114	14.522239	0.580557
-28.391884	23.180202	0.585562
-28.761493	22.511652	0.590566
-29.229685	21.291545	0.595571
-29.238471	12.228356	0.600576
-29.373006	15.644659	0.605581
-29.546605	29.022019	0.610586
-30.048784	13.771549	0.615590
-30.919796	18.422174	0.620595
-30.712607	15.205783	0.625600
-30.752621	15.739407	0.630605
-31.144119	8.925524	0.635610
-30.823519	15.118375	0.640614
-31.256233	18.330219	0.645619
-31.433305	24.505582	0.650624
-32.429707	17.771538	0.655629
-33.006481	26.054387	0.660634
-32.469162	26.089602	0.665638
-32.266796	18.669901	0.670643
-32.485628	8.526153	0.675648
-33.438016	19.500377	0.680653
-34.171395	26.931687	0.685658
-34.183322	12.718827	0.690662
-34.181599	14.264738	0.695667
-34.255892	23.583469	0.700672
-34.263113	23.338035	0.705677
-34.424883	19.118842	0.710682
-34.657173	25.214838	0.715686
-35.623134	26.726031	0.720691
-35.609173	13.565271	0.725696
-35.773842	15.978121	0.730701
-36.234333	27.093422	0.735706
-35.999607	16.665568	0.740710
-36.348648	20.019457	0.745715
-36.578129	15.151465	0.750720
-37.187267	13.358591	0.755725
-37.359461	31.330787	0.760730
-37.381692	22.822272	0.765734
-37.477269	16.445250	0.770739
-38.193699	18.040000	0.775744
-38.645167	18.371313	0.780749
-39.044222	13.446011	0.785754
-38.684709	18.192392	0.790758
-38.919245	20.667398	0.795763
-38.985288	12.056034	0.800768
-38.731182	11.894182	0.805773
-39.730315	10.641564	0.810778
-40.284888	10.257418	0.815782
-40.385593	15.487884	0.820787
-40.848011	14.839112	0.825792
-40.512769	4.891768	0.830797
-41.173959	18.380479	0.835802
-41.593977	16.459670	0.840806
-41.692270	13.562101	0.845811
-41.922521	17.861877	0.850816
-41.782164	16.159709	0.855821
-42.533131	18.330679	0.860826
-42.160672	12.079731	0.865830
-42.773994	16.018112	0.870835
-43.575219	14.115318	0.875840
-43.906777	15.295455	0.880845
-44.137474	18.677140	0.885850
-43.859734	7.307643	0.890854
-44.362200	12.054613	0.895859
-44.161463	6.443105	0.900864
-44.092082	13.830923	0.905869
-44.572066	6.571449	0.910874
-44.687757	3.508456	0.915878
-45.390556	11.345101	0.920883
-45.648834	-0.054386	0.925888
-45.635954	14.631159	0.930893
-45.779036	14.395946	0.935898
-46.121897	7.458603	0.940902
-47.144560	17.632426	0.945907
-47.078400	17.113533	0.950912
-47.162874	8.305248	0.955917
-47.548345	23.422835	0.960922
-47.312846	14.038213	0.965926
-47.263395	16.143492	0.970931
-47.603537	16.596692	0.975936
-48.409344	16.238084	0.980941
-48.656999	16.236499	0.985946
-48.391683	8.337897	0.990950
-48.854988	18.973709	0.995955
-49.716354	19.384899	1.000960
-49.759504	6.776967	1.005965
-50.769708	0.344430	1.010970
-50.549542	14.184789	1.015974
-50.446813	11.633025	1.020979
-50.435938	12.096482	1.025984
-50.315199	10.701803	1.030989
-50.592514	17.291399	1.035994
-51.061306	9.401951	1.040998
-51.551169	18.100363	1.046003
-51.774583	23.567458	1.051008
-51.711870	11.009111	1.056013
-52.055300	18.695016	1.061018
-52.921017	12.937849	1.066022
-53.316969	10.395102	1.071027
-53.537495	18.520517	1.076032
-53.009587	3.630480	1.081037
-53.610043	11.785731	1.086042
-53.398072	20.778058	1.091046
-53.840345	11.073942	1.096051
-54.716481	10.250562	1.101056
-54.756179	12.231671	1.106061
-54.754502	15.123909	1.111066
-54.925358	4.567070	1.116070
-55.208579	10.847376	1.121075
-55.050361	10.511068	1.126080
-55.636195	6.430231	1.131085
-56.374008	15.291160	1.136090
-56.205591	10.047543	1.141094
-56.767635	6.361530	1.146099
-56.895648	15.270546	1.151104
-56.536831	14.300980	1.156109
-57.625215	17.078396	1.161114
-58.058140	13.044106	1.166118
-58.256450	17.241922	1.171123
-58.334595	12.916079	1.176128
-58.170311	19.365709	1.181133
-58.224694	19.307520	1.186138
-58.480336	14.171275	1.191142
-59.535189	17.300571	1.196147
-60.085488	18.208371	1.201152
-60.068214	2.584003	1.206157
-60.291513	19.079011	1.211162
-60.226013	9.964877	1.216166
-60.290517	16.293782	1.221171
-60.420181	17.160279	1.226176
-60.001123	10.558516	1.231181
-60.517113	17.013830	1.236186
-60.732679	12.844471	1.241190
-61.115164	16.132561	1.246195
-61.918459	12.065762	1.251200
-62.392292	5.470295	1.256205
-62.943495	18.309547	1.261210
-63.052634	7.575783	1.266214
-62.947753	8.782346	1.271219
-63.105132	12.973791	1.276224
-62.960920	9.879287	1.281229
-63.320669	17.396035	1.286234
-63.269240	14.260336	1.291238
-63.775475	9.465513	1.296243
-64.296487	16.515646	1.301248
-64.687977	8.530161	1.306253
-65.321842	9.521224	1.311258
-65.741331	15.520103	1.316262
-65.625132	13.638038	1.321267
-65.511967	8.682938	1.326272
-65.951972	6.777965	1.331277
-66.268890	15.883544	1.336282
-66.090404	13.586609	1.341286
-66.386889	17.620510	1.346291
-66.477309	18.796607	1.351296
-67.009272	16.564800	1.356301
-67.472477	17.219368	1.361306
-67.767695	11.348090	1.366310
-67.744980	8.250976	1.371315
-68.081843	15.943390	1.376320
-68.231744	12.646323	1.381325
-69.661005	12.696876	1.386330
-69.267571	17.400553	1.391334
-68.795968	11.687257	1.396339
-69.579686	10.292498	1.401344
-69.742245	11.793938	1.406349
-69.910757	13.369365	1.411354
-69.707962	6.830770	1.416358
-70.142277	9.104689	1.421363
-70.786605	8.722356	1.426368
-70.860690	8.800506	1.431373
-71.614986	11.416065	1.436378
-71.784277	5.863937	1.441382
-71.998910	11.169264	1.446387
-71.992152	13.076005	1.451392
-71.629521	3.402931	1.456397
-71.825090	13.059555	1.461402
-72.932454	20.456287	1.466406
-73.203615	12.344271	1.471411
-73.390339	14.033397	1.476416
-73.185671	5.611304	1.481421
-73.415172	7.241105	1.486426
-73.280936	2.948828	1.491430
-73.990860	6.740002	1.496435
-74.433436	9.721938	1.501440
-74.794803	3.748737	1.506445
-75.110784	12.098377	1.511450
-74.828039	10.966076	1.516454
-75.041680	-0.245747	1.521459
-75.984509	8.111501	1.526464
-76.194179	1.111705	1.531469
-76.235810	6.986375	1.536474
-76.306339	0.402786	1.541478
-76.020087	4.818744	1.546483
-77.030475	12.005592	1.551488
-77.309331	5.016241	1.556493
-77.875302	7.708011	1.561498
-77.718792	-1.576732	1.566502
-77.628919	15.645278	1.571507
-77.697481	12.792716	1.576512
-77.954762	11.144330	1.581517
-78.883971	19.341784	1.586522
-79.266344	19.645205	1.591526
-79.208552	4.624509	1.596531
-79.515030	15.525425	1.601536
-79.510817	15.853151	1.606541
-79.698379	8.597639	1.611546
-80.305856	17.625654	1.616550
-80.496025	16.879111	1.621555
-81.139271	12.360471	1.626560
-81.231475	15.611931	1.631565
-81.743649	18.299744	1.636570
-81.293989	3.279495	1.641574
-81.239598	14.501866	1.646579
-81.717737	18.667994	1.651584
-81.420129	5.544618	1.656589
-82.467111	5.591778	1.661594
-82.763704	11.112199	1.666598
-83.350633	11.392900	1.671603
-83.073067	11.055315	1.676608
-82.773134	8.465632	1.681613
-83.586790	9.389336	1.686618
-84.349352	8.637359	1.691622
-84.986364	21.218906	1.696627
-85.198568	20.312931	1.701632
-84.686185	3.553322	1.706637
-85.243084	15.225558	1.711642
-84.763914	3.412775	1.716646
-84.826052	10.003701	1.721651
-85.283031	12.801958	1.726656
-85.427332	17.980141	1.731661
-85.967048	9.692221	1.736666
-86.231920	1.670032	1.741670
-86.349166	10.274103	1.746675
-87.326642	23.608609	1.751680
-87.771822	11.416454	1.756685
-87.517477	13.018970	1.761690
-88.148442	11.024117	1.766694
-87.645467	10.742703	1.771699
-87.943966	14.689134	1.776704
-87.581434	6.713895	1.781709
-88.869948	11.371077	1.786714
-89.080234	12.997999	1.791718
-89.367905	4.696640	1.796723
-89.514705	20.695701	1.801728
-89.250063	2.538971	1.806733
-89.675381	13.304641	1.811738
-90.278713	18.343427	1.816742
-90.673134	5.625748	1.821747
-90.949072	15.660672	1.826752
-90.954632	15.137650	1.831757
-91.238753	15.523191	1.836762
-91.058070	12.732627	1.841766
-91.169157	7.217247	1.846771
-92.534317	7.260467	1.851776
-92.506785	11.559464	1.856781
-92.912602	18.034847	1.861786
-92.863303	12.679215	1.866790
-93.210636	11.067022	1.871795
-93.167678	15.000427	1.876800
-92.787945	11.620859	1.881805
-93.319852	20.933529	1.886810
-93.904176	19.879812	1.891814
-94.351957	5.263890	1.896819
-94.365914	11.075189	1.901824
-94.019732	3.247279	1.906829
-95.201058	16.842273	1.911834
-95.427326	0.838001	1.916838
-95.725047	4.265387	1.921843
-96.230980	16.735294	1.926848
-96.055906	7.098742	1.931853
-96.055868	-6.697582	1.936858
-95.763968	2.850254	1.941862
-96.177243	9.771199	1.946867
-96.999966	6.956072	1.951872
-97.345796	-0.116517	1.956877
-97.528627	2.106565	1.961882
-97.511925	3.322373	1.966886
-97.733103	2.936699	1.971891
-98.884070	-2.268107	1.976896
-98.748553	-0.542565	1.981901
-99.230585	5.443167	1.986906
-99.143969	0.740769	1.991910
-99.354048	1.115256	1.996915
-99.476798	3.164837	2.006912
-98.778614	3.333349	2.016909
-98.313982	3.523076	2.026906
-98.011905	1.099841	2.036902
-98.027015	9.274463	2.046899
-97.405403	7.092334	2.056896
-96.841486	-0.131091	2.066893
-96.071601	2.756325	2.076890
-94.999604	5.102877	2.086886
-95.071468	4.244619	2.096883
-95.303586	9.438090	2.106880
-94.468639	9.739774	2.116877
-93.765116	3.450446	2.126874
-92.499282	5.838406	2.136870
-92.707059	5.500408	2.146867
-91.993763	-0.227936	2.156864
-91.634493	8.612765	2.166861
-91.483569	5.502114	2.176858
-90.734068	4.436739	2.186854
-90.362217	6.378441	2.196851
-89.350536	10.578729	2.206848
-88.850131	7.478872	2.216845
-88.739368	11.149147	2.226842
-88.355118	12.229469	2.236838
-87.505548	6.744910	2.246835
-87.301266	5.663110	2.256832
-86.238893	10.515658	2.266829
-85.581835	6.207571	2.276826
-85.819433	12.645531	2.286822
-85.549963	7.185132	2.296819
-84.611487	13.879748	2.306816
-84.134406	13.503685	2.316813
-83.838357	13.530927	2.326810
-82.776472	14.676121	2.336806
-82.594745	9.382391	2.346803
-82.567967	5.922774	2.356800
-81.561952	17.179023	2.366797
-81.117950	17.021149	2.376794
-80.710344	14.414571	2.386790
-79.760085	19.615774	2.396787
-79.475201	13.212494	2.406784
-79.474450	12.072961	2.416781
-78.230410	10.205901	2.426778
-78.363243	2.840750	2.436774
-77.728215	5.719836	2.446771
-77.039034	8.466300	2.456768
-76.908201	11.816622	2.466765
-76.027310	12.400189	2.476762
-75.193645	7.108409	2.486758
-75.058446	12.485753	2.496755
-74.931433	11.707382	2.506752
-74.275966	14.995595	2.516749
-73.361858	11.348729	2.526746
-73.121664	12.196873	2.536742
-72.038667	8.015309	2.546739
-71.876059	10.907081	2.556736
-72.090535	15.560772	2.566733
-71.508855	11.308803	2.576730
-70.734001	6.202175	2.586726
-69.975268	5.046474	2.596723
-69.097740	4.699009	2.606720
-69.393924	13.470091	2.616717
-69.089874	12.613616	2.626714
-67.646632	14.955618	2.636710
-67.448300	14.925716	2.646707
-67.337742	10.607588	2.656704
-66.228815	11.993095	2.666701
-65.940728	7.491581	2.676698
-65.816719	7.755929	2.686694
-65.235237	7.036246	2.696691
-64.321124	4.413526	2.706688
-64.487875	10.343115	2.716685
-63.466561	10.422717	2.726682
-62.787317	7.193241	2.736678
-62.705439	2.493924	2.746675
-62.250643	6.215802	2.756672
-61.165042	6.353332	2.766669
-61.172335	12.599728	2.776666
-60.681272	-1.820823	2.786662
-59.707920	10.800622	2.796659
-59.552527	6.081302	2.806656
-59.413321	5.406511	2.816653
-58.344350	12.367656	2.826650
-57.902614	13.494833	2.836646
-57.854110	4.962513	2.846643
-56.769136	10.413936	2.856640
-56.627141	10.637083	2.866637
-56.320369	9.530592	2.876634
-55.131911	10.849862	2.886630
-54.532713	13.105501	2.896627
-54.624080	14.568570	2.906624
-54.484674	13.277363	2.916621
-53.769070	9.094732	2.926618
-53.129833	9.254618	2.936614
-52.196221	10.149965	2.946611
-51.783893	2.413837	2.956608
-51.850096	11.832143	2.966605
-51.391715	9.206508	2.976602
-50.320573	5.272966	2.986598
-50.097920	6.826776	2.996595
-49.521966	4.963006	3.006592
-48.595934	6.811297	3.016589
-48.578228	9.424554	3.026586
-48.190007	12.304675	3.036582
-47.566726	-0.450329	3.046579
-47.060734	19.852598	3.056576
-46.772040	4.239583	3.066573
-45.633704	13.115169	3.076570
-45.439600	6.087248	3.086566
-45.370370	4.882415	3.096563
-44.406588	10.055259	3.106560
-43.756863	4.940915	3.116557
-43.552534	5.786443	3.126554
-43.288504	5.787912	3.136550
-41.988942	4.368192	3.146547
-41.890185	6.754148	3.156544
-42.194234	12.330721	3.166541
-40.760670	5.998780	3.176538
-40.326620	10.199071	3.186534
-40.209705	8.756201	3.196531
-39.174766	12.416137	3.206528
-38.711607	12.844022	3.216525
-38.661610	8.778999	3.226522
-38.415337	11.693395	3.236518
-37.429749	9.811565	3.246515
-37.197800	13.947614	3.256512
-36.313858	14.059752	3.266509
-35.539227	7.612133	3.276506
-34.981833	10.258984	3.286502
-35.220804	9.390113	3.296499
-34.848602	11.943502	3.306496
-34.173414	10.231407	3.316493
-33.693208	8.535089	3.326490
-32.843369	9.456334	3.336486
-32.404603	6.860563	3.346483
-31.975311	8.381410	3.356480
-31.340014	10.475310	3.366477
-30.677507	5.912166	3.376474
-30.721373	1.957880	3.386470
-30.083339	0.552561	3.396467
-28.963488	7.198345	3.406464
-29.099175	7.298174	3.416461
-28.810282	9.031436	3.426458
-28.045634	-0.484050	3.436454
-27.595436	6.505275	3.446451
-27.228697	8.399721	3.456448
-26.474845	5.651025	3.466445
-26.100427	6.795552	3.476442
-25.208187	3.704682	3.486438
-24.913009	1.686646	3.496435
-24.847155	11.690130	3.506432
-23.516745	8.394482	3.516429
-23.109326	9.001530	3.526426
-23.081180	13.884547	3.536422
-22.568426	11.091880	3.546419
-22.179042	9.419264	3.556416
-21.501361	6.725286	3.566413
-21.063313	3.342215	3.576410
-20.172522	11.928300	3.586406
-19.796015	8.810742	3.596403
-19.786650	2.300038	3.606400
-19.077453	15.404820	3.616397
-18.451707	7.717134	3.626394
-17.949483	4.735169	3.636390
-16.804246	13.691117	3.646387
-16.887095	11.981415	3.656384
-16.485955	19.244226	3.666381
-16.336066	10.598191	3.676378
-15.776070	6.198133	3.686374
-14.842234	1.462084	3.696371
-13.817495	3.846047	3.706368
-14.046543	9.021725	3.716365
-13.311943	1.441454	3.726362
-13.066941	6.016889	3.736358
-12.903800	1.944281	3.746355
-12.119939	4.238699	3.756352
-11.094452	7.754058	3.766349
-10.382922	13.378976	3.776346
-10.434780	8.721562	3.786342
-9.913050	14.474800	3.796339
-9.682725	12.805948	3.806336
-8.619664	5.027917	3.816333
-8.225945	13.961670	3.826330
-8.145977	7.072231	3.836326
-7.655013	10.634389	3.846323
-6.778752	13.333155	3.856320
-6.633951	3.766747	3.866317
-5.704345	13.678364	3.876314
-5.341971	15.535454	3.886310
-5.381958	16.256645	3.896307
-4.626590	22.720963	3.906304
-4.275602	33.510202	3.916301
-3.500438	36.077017	3.926298
-3.181669	40.787504	3.936294
-2.785811	49.380531	3.946291
-2.338141	67.503821	3.956288
-1.834736	74.809176	3.966285
-1.239388	88.944445	3.976282
-0.699644	98.017697	3.986278
-0.191871	107.516498	3.996275
0.000000	120.336213	4.001280
0.101125	123.136667	4.006285
0.342312	147.113724	4.011290
0.809307	147.392796	4.016294
0.930479	146.675293	4.021299
0.786974	157.892797	4.026304
1.154922	154.142433	4.031309
0.549092	163.758337	4.036314
0.955761	159.207802	4.041318
1.014504	154.607824	4.046323
0.785162	140.499137	4.051328
1.110386	152.885078	4.056333
0.731693	159.489221	4.061338
1.066779	150.858839	4.066342
1.142109	150.541555	4.071347
0.930256	166.204269	4.076352
1.234684	151.911174	4.081357
0.946409	161.872668	4.086362
1.210651	155.714918	4.091366
0.912158	148.867939	4.096371
0.661201	154.401193	4.101376
0.813481	159.623938	4.106381
0.641898	154.555533	4.111386
1.146561	162.344736	4.116390
1.099289	158.836620	4.121395
0.605427	160.261614	4.126400
1.200242	160.941703	4.131405
0.795201	158.230842	4.136410
0.820774	158.488943	4.141414
0.899498	154.947181	4.146419
0.886435	159.075060	4.151424
1.579141	147.316452	4.156429
0.928813	157.531531	4.161434
1.046235	158.979513	4.166438
1.055867	157.174629	4.171443
1.476565	166.218089	4.176448
1.316775	157.668203	4.181453
1.270304	162.218220	4.186458
1.418229	144.945694	4.191462
1.118641	152.865632	4.196467
1.095095	163.284442	4.201472
1.143732	149.059765	4.206477
1.207131	158.826405	4.211482
0.989324	164.967419	4.216486
1.803792	163.747040	4.221491
1.141265	167.187295	4.226496
1.604648	171.343579	4.231501
1.390868	171.701513	4.236506
1.458962	161.246738	4.241510
1.411194	152.415231	4.246515
1.239181	162.384247	4.251520
1.236026	155.017089	4.256525
1.252671	161.769586	4.261530
1.470234	171.666927	4.266534
1.541350	176.135758	4.271539
1.542991	181.962801	4.276544
1.413805	166.047458	4.281549
1.393014	171.014586	4.286554
1.517089	176.450355	4.291558
1.627632	177.132440	4.296563
1.371627	174.646343	4.301568
1.747163	166.753121	4.306573
1.404321	166.674529	4.311578
1.463748	173.187334	4.316582
1.874398	178.274653	4.321587
1.427959	168.906243	4.326592
1.652702	164.088920	4.331597
1.376886	174.674915	4.336602
1.739417	177.855210	4.341606
1.725892	169.573260	4.346611
1.610276	180.735563	4.351616
1.936865	167.717646	4.356621
1.547469	157.604054	4.361626
1.397687	154.033661	4.366630
1.432286	161.077968	4.371635
1.798657	180.180904	4.376640
2.345385	177.953807	4.381645
1.734291	166.445472	4.386650
1.682893	160.236591	4.391654
1.826166	165.039869	4.396659
1.498153	164.231351	4.401664
1.643548	168.697672	4.406669
1.808905	178.085316	4.411674
2.299005	177.572421	4.416678
1.851627	160.355935	4.421683
1.528344	154.299816	4.426688
1.677085	156.892041	4.431693
1.448481	178.430710	4.436698
1.995773	184.939255	4.441702
2.126583	176.654660	4.446707
1.841861	183.469104	4.451712
2.138125	174.514139	4.456717
2.046152	164.241490	4.461722
1.757220	169.121127	4.466726
1.828258	156.124242	4.471731
1.775556	177.148955	4.476736
2.367931	183.769914	4.481741
1.756427	180.556982	4.486746
1.987037	173.243623	4.491750
2.319044	177.275118	4.496755
1.706340	171.723196	4.501760
2.145055	177.449497	4.506765
2.179560	176.964144	4.511770
1.691337	167.600371	4.516774
1.841450	169.713405	4.521779
1.892833	170.511220	4.526784
2.306335	185.984879	4.531789
2.245673	199.886622	4.536794
2.275381	183.330485	4.541798
2.317668	187.040006	4.546803
2.067579	183.262336	4.551808
1.994439	181.860911	4.556813
1.946177	180.810628	4.561818
2.412098	184.002349	4.566822
2.411451	182.745311	4.571827
2.450980	178.164286	4.576832
1.952962	160.301991	4.581837
1.817789	170.722581	4.586842
2.200255	182.705851	4.591846
2.433964	181.248587	4.596851
2.574154	188.805822	4.601856
2.550802	168.877093	4.606861
2.009196	155.352532	4.611866
2.111010	169.898640	4.616870
2.663667	179.472172	4.621875
2.211753	177.437139	4.626880
2.029367	176.586501	4.631885
2.092368	170.971551	4.636890
2.428181	181.704492	4.641894
2.250937	177.538616	4.646899
2.435935	186.902795	4.651904
2.509533	177.061617	4.656909
2.116859	190.776813	4.661914
2.130666	174.653445	4.666918
2.009759	183.600851	4.671923
1.733205	194.345322	4.676928
2.318476	184.873390	4.681933
2.501358	190.411222	4.686938
2.875600	195.672670	4.691942
2.647707	179.684639	4.696947
2.381374	185.491251	4.701952
2.581994	184.294870	4.706957
2.285465	179.582924	4.711962
2.378357	174.719020	4.716966
2.456089	178.116065	4.721971
2.701027	198.013428	4.726976
2.756241	189.809489	4.731981
2.553806	190.880200	4.736986
2.687658	177.027350	4.741990
2.400782	182.628111	4.746995
2.206011	192.867570	4.752000
2.978366	200.793290	4.757005
2.806466	199.398812	4.762010
2.854965	197.853571	4.767014
2.618012	182.804151	4.772019
2.609107	182.548240	4.777024
2.729031	182.126707	4.782029
2.902254	193.986423	4.787034
2.700382	192.604988	4.792038
2.736380	189.217175	4.797043
2.633077	194.191533	4.802048
2.799681	182.829319	4.807053
2.988961	198.815559	4.812058
3.117522	199.054175	4.817062
2.734771	180.148184	4.822067
2.387744	184.808845	4.827072
2.556738	192.204067	4.832077
2.625693	200.268029	4.837082
3.032909	202.889170	4.842086
3.249991	208.403303	4.847091
2.876748	199.709117	4.852096
3.255191	204.362558	4.857101
2.817766	194.440276	4.862106
2.383663	194.514685	4.867110
3.045603	207.638107	4.872115
3.047535	214.622627	4.877120
3.444734	208.122553	4.882125
3.246049	196.796130	4.887130
2.880050	181.283250	4.892134
2.772354	179.484632	4.897139
2.659653	184.310684	4.902144
2.857576	198.071039	4.907149
2.801836	209.312059	4.912154
2.676588	219.400845	4.917158
3.294443	215.875139	4.922163
3.008473	209.870151	4.927168
3.046342	217.077710	4.932173
3.100695	225.524313	4.937178
2.780495	218.950413	4.942182
2.970005	218.281892	4.947187
3.112485	238.036123	4.952192
2.734999	217.228241	4.957197
2.628853	215.319560	4.962202
3.102449	225.428463	4.967206
3.519842	220.944209	4.972211
3.010114	222.737936	4.977216
3.062819	222.172525	4.982221
3.107416	236.130009	4.987226
3.225569	236.153503	4.992230
3.434744	236.703174	4.997235
3.419940	237.393348	5.002240
3.553770	234.445339	5.007245
3.206095	223.459016	5.012250
2.881002	224.617676	5.017254
3.426032	236.158591	5.022259
3.460832	239.382600	5.027264
3.508300	221.813361	5.032269
3.150950	218.772895	5.037274
3.010797	215.635568	5.042278
3.566093	223.771592	5.047283
3.523675	245.199380	5.052288
3.685159	241.276137	5.057293
3.013734	218.542552	5.062298
3.161444	233.889216	5.067302
3.429146	228.569626	5.072307
3.108116	241.474616	5.077312
3.248978	247.056506	5.082317
3.512115	243.856966	5.087322
3.282562	248.286125	5.092326
3.621896	250.171578	5.097331
3.662136	234.282129	5.102336
3.557884	234.619695	5.107341
3.783623	247.159874	5.112346
4.166669	238.447527	5.117350
3.655385	243.874766	5.122355
3.535186	246.312859	5.127360
3.394235	232.235552	5.132365
3.693845	247.630032	5.137370
3.459743	245.203247	5.142374
3.760033	233.990068	5.147379
3.614059	245.106923	5.152384
3.732808	237.514772	5.157389
3.521299	239.541864	5.162394
3.752103	240.572257	5.167398
3.632843	236.152119	5.172403
3.561683	241.980956	5.177408
3.942811	248.962611	5.182413
3.646955	248.023779	5.187418
3.416629	248.508655	5.192422
3.686839	240.668513	5.197427
3.477031	246.832703	5.202432
3.606628	238.469648	5.207437
3.518958	247.892540	5.212442
3.366509	244.521355	5.217446
3.593199	241.553955	5.222451
3.405676	250.721260	5.227456
3.556746	256.502130	5.232461
3.914596	273.176034	5.237466
3.599454	273.962112	5.242470
4.082816	270.877410	5.247475
4.041155	284.443426	5.252480
4.210840	263.300196	5.257485
4.181134	270.582086	5.262490
3.726341	264.911199	5.267494
3.975621	260.647586	5.272499
3.930952	269.180819	5.277504
3.991988	269.421913	5.282509
3.933476	272.391530	5.287514
3.987196	275.405147	5.292518
4.004839	274.889824	5.297523
4.185477	279.353214	5.302528
3.944220	258.992359	5.307533
3.795085	265.628261	5.312538
4.407647	267.889820	5.317542
3.950719	260.657582	5.322547
3.998947	273.909908	5.327552
4.149348	267.596604	5.332557
4.341307	267.376259	5.337562
3.882257	269.434496	5.342566
4.017346	271.293131	5.347571
3.932494	285.717676	5.352576
4.064238	270.903797	5.357581
4.104894	275.486704	5.362586
3.798509	278.031535	5.367590
3.959335	277.343680	5.372595
3.677255	285.586057	5.377600
4.098617	277.007051	5.382605
4.233898	278.895448	5.387610
3.805750	279.533376	5.392614
4.041003	279.896918	5.397619
4.245369	285.815790	5.402624
4.239409	294.527717	5.407629
4.016126	302.565247	5.412634
4.318622	305.593991	5.417638
4.635704	288.763441	5.422643
4.400155	302.275782	5.427648
4.619245	299.635485	5.432653
4.488603	284.003892	5.437658
4.388826	279.798550	5.442662
4.263557	279.685383	5.447667
4.272348	275.638988	5.452672
4.187468	274.118938	5.457677
4.382623	291.117094	5.462682
4.423214	299.954614	5.467686
4.670464	290.775349	5.472691
4.693053	305.147628	5.477696
4.837787	282.802634	5.482701
4.632778	272.743732	5.487706
4.175389	284.751533	5.492710
4.274999	281.538757	5.497715
4.100923	272.889652	5.502720
4.565060	290.303383	5.507725
4.482881	307.070562	5.512730
4.561844	303.809005	5.517734
4.744704	297.233526	5.522739
4.421226	308.729492	5.527744
4.650863	294.264732	5.532749
4.576149	302.919856	5.537754
4.224400	307.374848	5.542758
4.427093	299.523045	5.547763
4.620170	312.635844	5.552768
4.582900	295.890187	5.557773
4.739866	305.528794	5.562778
4.583564	311.191485	5.567782
4.696552	299.859157	5.572787
4.597454	305.494239	5.577792
4.583687	308.449759	5.582797
4.883867	307.956408	5.587802
4.532008	304.903178	5.592806
4.419158	301.321221	5.597811
4.812619	308.482390	5.602816
4.722401	305.458829	5.607821
4.711599	309.677334	5.612826
4.760819	299.685415	5.617830
4.806490	309.778374	5.622835
4.215658	311.678349	5.627840
4.810993	321.501914	5.632845
5.019910	322.125523	5.637850
4.655814	333.456561	5.642854
4.845764	322.853582	5.647859
5.013581	330.438089	5.652864
5.200792	323.024691	5.657869
4.788020	301.960497	5.662874
4.810468	316.546596	5.667878
5.191857	317.381435	5.672883
4.679117	318.934952	5.677888
5.111384	325.170251	5.682893
4.894830	323.010374	5.687898
5.140251	315.963829	5.692902
4.940943	308.135737	5.697907
4.999592	323.184372	5.702912
5.182923	321.970022	5.707917
5.053554	315.920072	5.712922
4.884391	311.975390	5.717926
5.532584	310.133231	5.722931
5.190526	310.773506	5.727936
4.937436	310.256456	5.732941
5.327478	302.138399	5.737946
4.777196	308.458422	5.742950
5.206351	303.103444	5.747955
4.724104	314.087687	5.752960
5.369679	327.082706	5.757965
5.141670	327.891185	5.762970
5.053903	323.391136	5.767974
5.239376	327.885015	5.772979
5.197693	339.565585	5.777984
5.494920	341.309827	5.782989
5.528209	320.607653	5.787994
5.229726	313.732876	5.792998
5.355773	310.431178	5.798003
5.166109	310.369693	5.803008
5.183322	304.432851	5.808013
4.898496	308.199913	5.813018
5.121629	322.774162	5.818022
5.413684	322.763492	5.823027
5.396044	339.899173	5.828032
5.473373	337.196071	5.833037
5.715531	340.209439	5.838042
5.063220	329.106754	5.843046
5.425381	319.111250	5.848051
5.198572	324.815884	5.853056
5.275573	338.914216	5.858061
5.418216	328.370647	5.863066
5.139124	337.517621	5.868070
5.399005	328.385081	5.873075
5.054836	338.937104	5.878080
4.899808	337.235177	5.883085
4.643498	334.883966	5.888090
5.128696	344.367234	5.893094
5.735588	355.228541	5.898099
5.919721	367.507648	5.903104
5.396460	347.592538	5.908109
5.675177	348.926968	5.913114
5.247360	351.615000	5.918118
5.452669	347.794784	5.923123
5.444251	370.781013	5.928128
5.482137	363.254648	5.933133
5.757270	361.388304	5.938138
5.557817	374.880636	5.943142
5.767879	358.104791	5.948147
5.777653	372.071804	5.953152
5.562834	366.641009	5.958157
5.788604	373.064651	5.963162
5.839541	371.023838	5.968166
5.877163	365.815623	5.973171
5.456542	363.034689	5.978176
5.502818	356.545092	5.983181
5.540311	364.643048	5.988186
5.597021	378.151948	5.993190
5.683396	366.858202	5.998195
5.626477	373.488580	6.003200
5.590006	373.756543	6.008205
5.572162	360.508889	6.013210
5.462711	372.877361	6.018214
5.374814	375.607384	6.023219
5.406438	362.543438	6.028224
5.305705	376.089799	6.033229
5.688839	378.439208	6.038234
5.966633	390.766094	6.043238
6.063892	391.436473	6.048243
5.744315	380.711961	6.053248
5.696289	372.909347	6.058253
5.789991	376.730580	6.063258
5.772741	380.487970	6.068262
6.001099	364.445952	6.073267
5.975983	378.841377	6.078272
5.856136	368.913953	6.083277
6.152949	357.858319	6.088282
5.827911	375.551632	6.093286
5.897597	364.605743	6.098291
5.974067	367.679053	6.103296
5.572116	378.494394	6.108301
5.692251	378.395524	6.113306
5.173116	368.534875	6.118310
5.852704	361.969029	6.123315
5.920287	370.836264	6.128320
5.785745	371.662941	6.133325
5.810365	361.217680	6.138330
5.469647	374.213344	6.143334
5.931290	366.316445	6.148339
6.297469	376.772610	6.153344
5.888844	374.997161	6.158349
6.107722	359.890982	6.163354
5.640568	378.377790	6.168358
5.610742	375.929952	6.173363
5.352531	364.947782	6.178368
5.549808	367.223823	6.183373
6.139284	373.780232	6.188378
5.574371	366.455788	6.193382
5.813293	361.904995	6.198387
5.836881	373.165582	6.203392
5.951984	373.016440	6.208397
6.031724	365.061603	6.213402
5.865909	370.110376	6.218406
5.738286	368.447029	6.223411
5.532779	379.282391	6.228416
5.593955	360.768371	6.233421
5.889584	361.097273	6.238426
5.668311	381.113749	6.243430
5.909711	367.372588	6.248435
5.773785	368.058120	6.253440
5.800955	370.695037	6.258445
5.798940	364.156394	6.263450
5.441615	378.655553	6.268454
5.719173	368.317359	6.273459
5.946804	363.928352	6.278464
5.641221	371.008058	6.283469
5.802974	360.604656	6.288474
5.492721	371.884008	6.293478
5.967167	364.410396	6.298483
5.909502	368.974952	6.303488
5.451604	375.993804	6.308493
5.709428	365.823232	6.313498
5.615677	375.505783	6.318502
5.848110	363.200855	6.323507
5.567419	361.021285	6.328512
5.970057	368.989645	6.333517
5.872872	364.690917	6.338522
5.579286	367.661318	6.343526
5.425655	367.677044	6.348531
5.633574	364.378774	6.353536
5.503789	356.081999	6.358541
5.835782	367.816660	6.363546
5.713062	364.800036	6.368550
5.511601	371.742570	6.373555
6.180002	387.246427	6.378560
5.590039	380.148782	6.383565
5.583172	373.928312	6.388570
5.557466	402.646469	6.393574
5.929376	393.866815	6.398579
6.056586	400.632813	6.403584
5.941956	389.194886	6.408589
5.911337	375.160775	6.413594
5.679808	364.994714	6.418598
5.745320	376.359165	6.423603
5.899989	368.056614	6.428608
5.620509	367.558820	6.433613
6.136590	372.139549	6.438618
5.850755	378.072183	6.443622
5.843213	367.759005	6.448627
5.728319	382.298606	6.453632
5.648090	374.051938	6.458637
6.068048	366.967055	6.463642
5.766298	379.110609	6.468646
6.194094	373.580323	6.473651
6.000872	370.596757	6.478656
5.863551	373.715857	6.483661
5.690547	369.514205	6.488666
5.624729	367.567863	6.493670
5.764098	370.618053	6.498675
5.926772	363.935091	6.503680
5.967147	361.909935	6.508685
6.089761	365.409112	6.513690
5.866196	372.910335	6.518694
6.045547	363.340030	6.523699
5.815092	361.459371	6.528704
5.673901	342.946159	6.533709
5.935364	339.411053	6.538714
5.712580	343.810906	6.543718
5.569383	342.726874	6.548723
5.582521	350.317814	6.553728
5.690450	364.555094	6.558733
6.035627	367.824620	6.563738
5.788826	368.649723	6.568742
5.970777	352.582534	6.573747
5.530359	350.382303	6.578752
5.391516	354.529639	6.583757
5.904827	365.224103	6.588762
5.733704	372.879343	6.593766
5.784785	375.095095	6.598771
6.042663	368.039758	6.603776
5.706640	370.405115	6.608781
5.365124	362.230242	6.613786
5.480187	378.446667	6.618790
5.566466	366.339424	6.623795
5.623658	372.724036	6.628800
5.802435	376.493326	6.633805
6.145577	373.895063	6.638810
6.112925	367.096789	6.643814
5.904400	371.314148	6.648819
6.063020	372.371375	6.653824
5.759089	353.608218	6.658829
5.775650	348.339364	6.663834
5.185656	358.236701	6.668838
5.733853	353.799259	6.673843
5.945606	369.951257	6.678848
5.879253	375.528370	6.683853
6.025813	363.207740	6.688858
5.293722	365.556270	6.693862
5.664776	358.072420	6.698867
6.048258	366.929771	6.703872
5.803728	372.945157	6.708877
6.114194	369.338609	6.713882
5.687242	356.647601	6.718886
5.562657	346.864715	6.723891
5.739956	362.145155	6.728896
5.884584	363.300883	6.733901
5.858922	346.872303	6.738906
5.174754	361.976252	6.743910
5.869246	358.726121	6.748915
6.176105	365.701951	6.753920
5.766346	363.088218	6.758925
5.759580	348.082973	6.763930
5.567876	344.397919	6.768934
5.903153	354.354850	6.773939
5.873925	353.559493	6.778944
5.649980	357.800508	6.783949
5.913824	351.936344	6.788954
5.573280	351.560123	6.793958
5.756767	351.389716	6.798963
5.840730	372.845335	6.803968
5.725138	360.307579	6.808973
5.723118	353.776539	6.813978
5.954281	378.246820	6.818982
5.989594	361.511195	6.823987
5.823076	350.998773	6.828992
5.458221	355.485740	6.833997
5.508584	342.802187	6.839002
5.500835	353.265081	6.844006
6.028026	368.826685	6.849011
5.919588	369.109698	6.854016
5.880427	359.384706	6.859021
5.743227	352.089722	6.864026
5.490461	351.721883	6.869030
5.822712	348.357983	6.874035
5.650432	363.202720	6.879040
5.288264	368.734600	6.884045
5.992467	367.716915	6.889050
5.961590	367.501134	6.894054
5.798402	362.495300	6.899059
5.845479	368.859582	6.904064
5.825606	370.515746	6.909069
5.986741	365.205137	6.914074
5.684866	362.190497	6.919078
5.569429	348.139648	6.924083
5.617125	352.927013	6.929088
5.393740	363.993508	6.934093
5.945793	367.782698	6.939098
5.671729	363.873984	6.944102
5.895807	369.664043	6.949107
5.819447	377.615475	6.954112
5.452821	376.471188	6.959117
5.814368	361.651604	6.964122
5.826771	372.913644	6.969126
5.711193	373.463615	6.974131
5.878850	374.578148	6.979136
5.874059	365.212597	6.984141
5.595981	360.671376	6.989146
5.336432	362.268985	6.994150
5.628894	361.001871	6.999155
5.479828	368.808747	7.004160
5.690620	373.627471	7.009165
5.795266	355.750592	7.014170
5.292645	368.828156	7.019174
5.374661	360.301434	7.024179
5.692606	362.626591	7.029184
5.717892	378.988768	7.034189
5.868395	368.045799	7.039194
5.877639	371.625964	7.044198
5.485695	359.606339	7.049203
5.803719	372.363211	7.054208
5.325771	381.307187	7.059213
5.871327	386.626518	7.064218
6.263065	393.207325	7.069222
6.119112	386.231605	7.074227
5.902785	376.692545	7.079232
5.945542	384.487165	7.084237
6.261616	369.187137	7.089242
6.015992	378.139778	7.094246
5.852019	374.321980	7.099251
5.678544	371.472874	7.104256
5.615522	385.752730	7.109261
5.970450	373.927931	7.114266
5.784778	378.049962	7.119270
5.957223	376.385368	7.124275
5.649589	373.463722	7.129280
5.555696	368.014423	7.134285
5.912580	373.050414	7.139290
5.722803	369.962987	7.144294
6.024959	358.164876	7.149299
6.089374	368.314857	7.154304
5.729956	374.792981	7.159309
5.850005	361.075629	7.164314
5.741423	378.841104	7.169318
5.570301	372.428468	7.174323
5.754511	360.931409	7.179328
6.136980	379.955279	7.184333
5.842828	369.715707	7.189338
5.616907	367.679409	7.194342
5.818263	374.324522	7.199347
6.041271	373.422762	7.204352
5.787469	359.915669	7.209357
5.518020	349.335613	7.214362
5.397554	357.611993	7.219366
5.730412	363.879817	7.224371
5.666430	373.538998	7.229376
5.831313	374.698976	7.234381
5.916991	373.732206	7.239386
5.750568	378.424344	7.244390
5.948080	380.023472	7.249395
5.411958	377.995125	7.254400
5.710021	380.712373	7.259405
6.263540	384.199044	7.264410
5.833146	378.319964	7.269414
5.612519	381.690888	7.274419
6.250555	376.059364	7.279424
5.553357	365.823064	7.284429
5.748450	363.734160	7.289434
5.432682	368.981248	7.294438
5.862116	375.035312	7.299443
5.948329	371.659385	7.304448
5.747255	370.343112	7.309453
5.687928	354.723932	7.314458
5.571432	359.862121	7.319462
5.521733	373.458450	7.324467
5.805726	383.105809	7.329472
5.561447	387.463253	7.334477
5.841596	379.593972	7.339482
5.943730	388.225640	7.344486
5.928293	380.281492	7.349491
5.858845	379.359201	7.354496
5.888586	385.133237	7.359501
5.796905	363.863670	7.364506
5.482863	363.617338	7.369510
5.545771	371.894005	7.374515
6.191430	376.771979	7.379520
6.045939	368.291038	7.384525
5.910471	350.060112	7.389530
5.954641	344.842536	7.394534
6.060294	355.495446	7.399539
6.107453	351.824092	7.404544
5.390087	345.609863	7.409549
5.806963	355.025011	7.414554
5.763470	358.897522	7.419558
5.534539	348.632881	7.424563
5.471000	348.987398	7.429568
5.443372	346.726844	7.434573
5.656012	334.677174	7.439578
5.634605	350.806418	7.444582
5.909653	359.299296	7.449587
5.877368	362.177581	7.454592
5.734257	353.927898	7.459597
5.933506	345.861276	7.464602
5.725513	354.068065	7.469606
5.692425	346.333140	7.474611
5.823005	344.155357	7.479616
5.743843	347.078973	7.484621
5.666377	342.638382	7.489626
5.652169	358.092529	7.494630
5.730037	357.769396	7.499635
6.078877	365.399772	7.504640
6.051750	356.305866	7.509645
5.672436	345.291831	7.514650
5.697258	357.559374	7.519654
5.697479	350.191169	7.524659
6.059313	357.318028	7.529664
5.635190	352.490279	7.534669
6.097181	357.813247	7.539674
5.938551	351.336205	7.544678
5.906213	337.028843	7.549683
5.988567	353.568217	7.554688
5.667295	356.923508	7.559693
5.685954	349.434068	7.564698
5.748922	348.347437	7.569702
5.590205	346.158959	7.574707
5.773073	349.483618	7.579712
5.671042	358.282292	7.584717
5.877245	342.238631	7.589722
5.750367	337.849122	7.594726
5.661392	349.566224	7.599731
5.843154	346.573573	7.604736
5.624890	350.520050	7.609741
5.741717	340.405944	7.614746
5.453826	352.333401	7.619750
5.236216	348.895616	7.624755
5.504591	346.715877	7.629760
5.550312	370.481118	7.634765
6.003406	371.060826	7.639770
5.812093	386.927448	7.644774
5.905872	378.162394	7.649779
5.848654	365.743732	7.654784
5.501173	376.198166	7.659789
5.777128	374.044004	7.664794
5.870827	375.632072	7.669798
5.764520	382.916316	7.674803
6.152057	373.481189	7.679808
5.604837	365.566328	7.684813
5.411616	356.508157	7.689818
5.720030	366.241246	7.694822
6.005340	368.777593	7.699827
6.130465	366.232920	7.704832
5.659599	369.881476	7.709837
5.654718	360.332541	7.714842
5.824711	348.955438	7.719846
5.862779	337.636055	7.724851
5.805100	351.173701	7.729856
5.660528	347.694939	7.734861
5.893673	335.270543	7.739866
5.514081	353.772743	7.744870
5.379790	349.106346	7.749875
5.794884	356.423687	7.754880
5.821381	376.705338	7.759885
6.131233	366.996064	7.764890
5.954282	354.707199	7.769894
5.784171	358.590671	7.774899
5.614084	347.732561	7.779904
5.376591	347.243318	7.784909
5.976991	358.349083	7.789914
5.502641	372.711897	7.794918
6.001302	373.949013	7.799923
6.350321	368.201683	7.804928
5.685582	358.982291	7.809933
5.795138	350.931869	7.814938
5.354380	351.166114	7.819942
5.451353	348.113385	7.824947
5.870685	361.480559	7.829952
5.720012	365.647710	7.834957
6.012447	366.979677	7.839962
5.722311	364.722645	7.844966
5.779155	343.820124	7.849971
5.690979	348.891772	7.854976
5.771553	360.135829	7.859981
5.966841	349.757673	7.864986
5.814457	354.278783	7.869990
5.331837	360.710669	7.874995
6.043858	349.127282	7.880000
5.814471	365.770376	7.885005
5.937194	355.034645	7.890010
5.611973	350.305881	7.895014
5.846712	350.173076	7.900019
5.884244	342.863625	7.905024
5.422576	345.366253	7.910029
5.555943	347.278751	7.915034
5.849001	369.726814	7.920038
5.902664	365.473104	7.925043
6.167453	351.784424	7.930048
5.900988	358.742233	7.935053
5.778502	349.616142	7.940058
5.352155	352.315079	7.945062
5.518766	355.973414	7.950067
6.053181	348.758933	7.955072
5.411712	349.363254	7.960077
5.679001	364.496528	7.965082
6.149755	377.644786	7.970086
5.981201	364.462976	7.975091
5.978307	360.535594	7.980096
5.824560	351.455413	7.985101
5.889517	346.395012	7.990106
5.582697	353.432196	7.995110
5.574270	349.255147	8.000115
5.685311	337.954947	8.005133
5.735451	358.618618	8.010150
5.767132	349.529548	8.015168
5.864231	353.896112	8.020186
5.231512	348.511034	8.025203
5.361853	350.347461	8.030221
5.766721	373.454541	8.035238
5.866027	367.142361	8.040256
6.057022	374.345549	8.045274
5.846909	368.694409	8.050291
6.227504	372.772548	8.055309
5.741136	373.660136	8.060326
5.889615	358.538501	8.065344
5.942515	354.930158	8.070362
5.789640	362.052894	8.075379
5.801352	347.184234	8.080397
5.770781	353.645459	8.085414
5.777076	352.723268	8.090432
6.225588	359.136911	8.095450
5.970978	364.137853	8.100467
5.931675	345.561014	8.105485
5.603204	351.814733	8.110502
5.912720	350.055400	8.115520
5.804931	351.690976	8.120538
6.247825	345.887058	8.125555
6.182144	340.488770	8.130573
5.594091	357.676900	8.135590
5.884598	351.552569	8.140608
5.864915	348.214729	8.145626
5.494349	343.623942	8.150643
6.017070	348.257889	8.155661
5.787389	353.758830	8.160678
6.211698	361.761855	8.165696
6.256536	356.338213	8.170714
5.946756	348.621230	8.175731
5.648524	344.136869	8.180749
5.493113	346.173633	8.185766
5.997743	346.966039	8.190784
6.033569	360.935219	8.195802
6.006313	387.568590	8.200819
6.296883	370.187528	8.205837
6.179707	368.506776	8.210854
5.815169	356.057155	8.215872
5.906979	351.217060	8.220890
5.728552	349.538462	8.225907
6.067807	353.745349	8.230925
6.218895	368.795151	8.235942
6.090748	371.617497	8.240960
6.071432	345.399353	8.245978
6.005764	351.142420	8.250995
6.165840	356.082407	8.256013
5.651045	354.118132	8.261030
5.888542	358.791837	8.266048
6.033004	364.745112	8.271066
5.919056	369.972362	8.276083
6.405296	365.782574	8.281101
6.079221	378.926830	8.286118
5.682043	367.458267	8.291136
6.028012	357.666904	8.296154
6.233668	368.806177	8.301171
6.202607	370.908203	8.306189
6.070052	368.929173	8.311206
6.056941	368.708757	8.316224
6.134439	372.797229	8.321242
5.888897	371.714534	8.326259
6.236360	373.689847	8.331277
5.995460	379.287316	8.336294
5.971586	370.818502	8.341312
6.364386	373.624231	8.346330
6.191702	375.362246	8.351347
6.213522	368.777204	8.356365
5.939721	370.646175	8.361382
6.010518	364.795792	8.366400
6.143584	371.752408	8.371418
5.766512	389.774219	8.376435
6.051626	375.558231	8.381453
6.204462	371.375813	8.386470
6.292977	376.630126	8.391488
6.273199	378.857131	8.396506
5.784227	380.500990	8.401523
6.197852	367.380459	8.406541
6.000286	380.030353	8.411558
5.982205	380.005794	8.416576
6.390476	372.127724	8.421594
6.147150	369.280283	8.426611
6.278278	372.476030	8.431629
6.615780	378.066378	8.436646
6.305316	376.805771	8.441664
6.606003	375.668921	8.446682
6.151692	379.329153	8.451699
6.062430	371.071003	8.456717
5.913721	373.476169	8.461734
5.916808	381.561706	8.466752
6.173206	376.730518	8.471770
6.078478	390.468599	8.476787
6.280376	376.688318	8.481805
6.179427	371.467759	8.486822
6.041809	389.278776	8.491840
6.380120	378.971945	8.496858
6.192271	381.363212	8.501875
6.250832	383.209339	8.506893
6.277283	382.682745	8.511910
5.750521	373.018868	8.516928
6.050586	384.304524	8.521946
6.298348	404.359639	8.526963
6.465266	397.336817	8.531981
6.264155	403.876530	8.536998
6.278170	411.349778	8.542016
6.388390	407.955819	8.547034
6.647379	425.989267	8.552051
6.420737	409.343790	8.557069
6.255816	389.431945	8.562087
6.359624	383.315822	8.567104
6.071013	389.128515	8.572122
6.238565	415.905884	8.577139
6.280650	402.214181	8.582157
6.560922	401.395794	8.587175
5.887627	423.362805	8.592192
6.249425	395.965986	8.597210
6.418420	411.628091	8.602227
6.597165	412.836679	8.607245
6.313494	403.190373	8.612263
6.284436	403.533691	8.617280
6.448583	401.985344	8.622298
6.132010	413.809052	8.627315
6.316999	413.848256	8.632333
6.341028	409.336992	8.637351
6.385467	409.619357	8.642368
6.507578	403.196624	8.647386
6.180770	407.885172	8.652403
6.349222	410.019081	8.657421
6.226019	409.177231	8.662439
6.143516	399.608388	8.667456
6.730917	406.701703	8.672474
6.572494	408.835802	8.677491
6.621916	409.861179	8.682509
6.474175	409.203858	8.687527
6.105170	407.986675	8.692544
6.186146	404.891876	8.697562
6.288250	432.290096	8.702579
6.491887	436.603849	8.707597
6.552503	437.250588	8.712615
6.409638	447.065329	8.717632
6.322813	439.581083	8.722650
6.453120	439.873957	8.727667
6.776777	445.074378	8.732685
6.740680	438.860611	8.737703
6.565068	442.484247	8.742720
6.558562	437.995045	8.747738
6.510883	451.882262	8.752755
6.469640	436.244873	8.757773
6.540885	447.575081	8.762791
6.588305	444.615812	8.767808
6.547963	430.802301	8.772826
6.541818	442.032130	8.777843
6.598555	438.350314	8.782861
7.068527	437.763314	8.787879
6.940944	449.936544	8.792896
6.728146	439.740231	8.797914
6.795445	435.683522	8.802931
6.676222	433.275993	8.807949
6.784636	418.904658	8.812967
6.226362	416.163967	8.817984
6.690823	424.883168	8.823002
6.784423	439.973734	8.828019
6.810285	439.062868	8.833037
6.721656	426.657633	8.838055
6.586190	417.288140	8.843072
6.825587	417.808996	8.848090
6.768094	410.208032	8.853107
6.562254	398.400215	8.858125
6.623650	406.794072	8.863143
6.348799	427.156204	8.868160
6.957698	426.552938	8.873178
7.135762	433.897631	8.878195
6.828604	422.523675	8.883213
6.923357	405.890232	8.888231
6.742444	420.095536	8.893248
6.848143	412.708101	8.898266
6.777833	409.220381	8.903283
6.489260	412.423107	8.908301
6.838715	421.588090	8.913319
6.763725	418.494068	8.918336
6.944700	412.817446	8.923354
6.657616	412.169375	8.928371
6.581232	412.144119	8.933389
6.723116	406.697337	8.938407
6.324027	415.979917	8.943424
6.690126	430.223349	8.948442
6.890996	434.584202	8.953459
6.783756	441.447323	8.958477
6.991237	437.385848	8.963495
6.784564	441.828420	8.968512
6.746969	434.375993	8.973530
6.593656	435.146551	8.978547
6.777270	438.226771	8.983565
7.098166	436.449607	8.988583
6.730696	439.281895	8.993600
6.675813	431.554630	8.998618
6.986811	447.006828	9.003635
7.045268	446.778914	9.008653
6.860636	423.247333	9.013671
6.790679	438.997271	9.018688
6.568274	434.428517	9.023706
6.960284	433.012160	9.028723
6.612763	437.191749	9.033741
6.846933	438.296121	9.038759
6.831621	441.410298	9.043776
6.704431	433.853510	9.048794
6.551763	435.879303	9.053811
6.491447	444.036360	9.058829
6.793863	437.411216	9.063847
6.584765	444.889862	9.068864
6.900997	459.747240	9.073882
7.028798	465.114160	9.078899
6.855632	476.190747	9.083917
7.503991	470.974154	9.088935
7.274138	460.148989	9.093952
6.892520	450.931547	9.098970
6.869435	445.733128	9.103987
6.490241	443.367575	9.109005
7.034546	463.140543	9.114023
7.386634	470.232134	9.119040
7.044093	467.182809	9.124058
6.985413	456.278976	9.129075
7.061980	459.864878	9.134093
6.838887	443.901112	9.139111
6.987841	469.519002	9.144128
6.873581	479.044647	9.149146
7.310369	473.886338	9.154163
7.141888	466.064269	9.159181
7.243547	470.221201	9.164199
7.051295	452.174619	9.169216
6.702237	444.331725	9.174234
7.218608	467.522467	9.179251
6.984136	462.421068	9.184269
7.504946	460.389553	9.189287
7.244528	457.606029	9.194304
6.963896	438.251908	9.199322
7.261444	445.061716	9.204339
7.042919	456.300083	9.209357
7.169590	440.098243	9.214375
7.181308	444.036026	9.219392
7.220619	443.796417	9.224410
7.336641	441.816348	9.229427
6.889241	441.698993	9.234445
7.025210	433.095485	9.239463
7.292211	458.763322	9.244480
7.415421	460.562857	9.249498
7.404041	435.715399	9.254515
6.855317	442.419932	9.259533
7.334352	439.263773	9.264551
7.029793	440.854923	9.269568
6.994519	453.484847	9.274586
7.277754	449.772389	9.279603
7.511468	456.991288	9.284621
7.269370	455.151091	9.289639
7.260449	443.479953	9.294656
7.114790	432.333380	9.299674
7.345808	437.576759	9.304691
7.078229	438.947573	9.309709
7.319908	437.286726	9.314727
7.313067	444.786857	9.319744
7.186415	445.342719	9.324762
7.342100	445.455747	9.329779
7.352750	450.691365	9.334797
7.243530	434.085204	9.339815
7.205196	449.438573	9.344832
7.373537	453.016786	9.349850
7.401840	462.440925	9.354867
7.389006	457.973034	9.359885
7.352639	440.050182	9.364903
7.202485	451.659646	9.369920
7.339917	455.509643	9.374938
7.154485	455.513921	9.379955
7.133565	474.140318	9.384973
7.289463	480.308926	9.389991
7.351432	469.657233	9.395008
7.373374	465.438067	9.400026
7.051117	464.823557	9.405043
7.193231	470.827939	9.410061
7.715944	469.103031	9.415079
7.600131	469.501526	9.420096
7.487632	469.980558	9.425114
7.633430	463.707200	9.430131
7.541492	467.793882	9.435149
7.819623	463.844223	9.440167
7.638393	444.085266	9.445184
7.099893	443.270715	9.450202
7.325747	435.929245	9.455219
7.256222	458.040079	9.460237
7.440415	461.519042	9.465255
7.529225	475.258062	9.470272
7.337683	462.513089	9.475290
7.950203	457.067532	9.480307
7.486154	467.183341	9.485325
7.244822	446.963251	9.490343
7.430760	453.857044	9.495360
7.377247	464.783563	9.500378
7.657824	466.374454	9.505395
7.561726	473.256117	9.510413
7.601077	466.579080	9.515431
7.793387	457.760287	9.520448
7.459734	466.438017	9.525466
7.569002	452.686850	9.530483
7.337227	454.660772	9.535501
7.741421	463.169332	9.540519
7.553417	456.864348	9.545536
7.213933	466.403882	9.550554
7.907870	477.280692	9.555571
7.505478	467.646978	9.560589
7.862860	466.080271	9.565607
7.651589	466.645296	9.570624
7.470935	458.771022	9.575642
7.709376	453.725501	9.580659
7.396818	468.071673	9.585677
7.331316	457.299254	9.590695
8.033514	474.155910	9.595712
7.831425	474.839964	9.600730
7.747107	456.539074	9.605747
7.479513	470.048762	9.610765
7.661301	462.822609	9.615783
7.913553	467.785187	9.620800
7.576959	456.681564	9.625818
7.670490	448.916381	9.630835
7.327513	449.397484	9.635853
7.575466	461.830937	9.640871
7.855623	470.117629	9.645888
7.588229	469.611941	9.650906
7.731045	463.391230	9.655923
7.459629	481.735183	9.660941
7.596698	475.293417	9.665959
7.866620	465.282810	9.670976
7.836603	480.153343	9.675994
7.999881	476.097589	9.681011
7.914675	473.811571	9.686029
7.685462	475.728588	9.691047
7.973817	466.810864	9.696064
7.725787	473.959513	9.701082
8.049475	478.797321	9.706099
8.006610	459.237872	9.711117
7.459136	455.435870	9.716135
7.645194	462.148780	9.721152
7.864495	471.114778	9.726170
7.858514	465.193007	9.731187
7.890665	475.803768	9.736205
7.821188	476.474369	9.741223
7.960793	473.525052	9.746240
7.883792	476.984104	9.751258
7.930910	468.743513	9.756275
7.782902	467.215059	9.761293
7.771103	480.314156	9.766311
7.775311	475.856826	9.771328
7.724876	472.233256	9.776346
7.855218	476.302199	9.781363
7.958977	475.682134	9.786381
7.768739	481.053892	9.791399
7.868021	484.346835	9.796416
7.625843	486.454736	9.801434
7.906510	469.413120	9.806451
7.420251	482.884757	9.811469
7.748257	479.904304	9.816487
7.863899	473.079055	9.821504
7.811426	484.980997	9.826522
7.727482	477.912704	9.831539
7.898973	470.980117	9.836557
7.857677	475.832580	9.841575
8.111345	481.520563	9.846592
7.945064	483.120848	9.851610
7.925238	486.058750	9.856627
7.967607	494.899112	9.861645
7.906918	497.244387	9.866663
8.178039	484.142485	9.871680
7.781219	509.756363	9.876698
7.814313	503.629540	9.881715
7.523399	491.878713	9.886733
7.622940	503.709200	9.891751
7.627640	497.869592	9.896768
8.033618	500.805817	9.901786
7.890892	497.332306	9.906803
8.106790	498.698802	9.911821
7.857475	499.182338	9.916839
7.899798	514.151654	9.921856
8.254289	521.751132	9.926874
8.420134	505.833536	9.931891
7.841137	506.419675	9.936909
7.854931	508.805683	9.941927
8.368918	516.796627	9.946944
8.408397	527.784775	9.951962
8.486070	505.458182	9.956979
8.225869	499.792440	9.961997
8.060939	508.913965	9.967015
8.313783	491.295252	9.972032
7.885508	502.378690	9.977050
8.246709	503.318501	9.982067
7.982876	499.329880	9.987085
8.120675	506.451193	9.992103
8.232453	498.147549	9.997120
8.228262	516.621166	10.002138
8.186477	513.285073	10.007155
8.467870	506.625290	10.012173
8.313781	513.352218	10.017191
7.858261	503.847906	10.022208
7.816810	521.692484	10.027226
8.447695	531.793105	10.032243
8.524035	526.475886	10.037261
8.316290	531.265144	10.042279
8.529632	531.082484	10.047296
8.372248	517.607660	10.052314
8.417968	510.528059	10.057331
8.061814	508.331291	10.062349
8.158399	516.986561	10.067367
8.462889	525.081801	10.072384
8.405435	532.091721	10.077402
8.354744	515.140928	10.082419
8.268378	505.682674	10.087437
8.215714	521.062789	10.092455
8.747112	520.853547	10.097472
8.252874	501.444999	10.102490
8.178943	503.762352	10.107507
8.292161	516.237501	10.112525
8.358466	523.892477	10.117543
8.489589	518.486598	10.122560
8.545471	531.090698	10.127578
8.443969	528.300678	10.132595
8.612282	521.082137	10.137613
8.101520	507.257045	10.142631
8.405155	514.415706	10.147648
8.648831	533.330860	10.152666
8.555012	521.769735	10.157683
8.395902	512.824181	10.162701
8.461982	534.214435	10.167719
8.320478	529.846708	10.172736
8.424584	525.192577	10.177754
8.470581	537.466888	10.182771
8.927794	522.095392	10.187789
8.347098	524.297323	10.192807
8.679177	511.639462	10.197824
8.624587	510.801225	10.202842
8.548790	507.016321	10.207859
8.613194	498.416534	10.212877
8.335500	494.697275	10.217895
8.479442	504.312226	10.222912
8.582645	520.481176	10.227930
8.657952	523.745420	10.232947
8.762204	513.769048	10.237965
8.267020	514.290460	10.242983
8.339316	517.013876	10.248000
8.522876	517.626229	10.253018
8.454603	528.272909	10.258035
8.875766	524.469444	10.263053
8.656602	531.569952	10.268071
8.873451	527.988696	10.273088
8.572065	523.172786	10.278106
8.492378	540.269629	10.283123
8.944840	524.762428	10.288141
8.642817	533.987216	10.293159
8.481209	518.939398	10.298176
8.428217	527.481135	10.303194
8.915310	530.300340	10.308211
8.584561	536.488677	10.313229
8.753072	530.564320	10.318247
8.958096	533.736474	10.323264
9.133681	534.954254	10.328282
8.565048	516.963596	10.333299
8.841027	528.075225	10.338317
8.580408	530.376494	10.343335
8.822510	526.482369	10.348352
8.984688	534.618845	10.353370
8.713150	517.427438	10.358387
8.711831	512.095701	10.363405
8.536472	525.218520	10.368423
8.898798	542.315139	10.373440
8.647222	513.693174	10.378458
8.462178	524.907361	10.383475
8.921579	527.906303	10.388493
8.561859	536.212670	10.393511
8.814091	529.089487	10.398528
8.792068	529.933805	10.403546
8.441640	535.642816	10.408563
8.508750	517.520921	10.413581
8.519852	526.218468	10.418599
8.839905	523.490745	10.423616
8.734840	521.633798	10.428634
8.421754	531.358145	10.433651
8.559468	533.825724	10.438669
9.011738	548.906031	10.443687
9.122016	547.976978	10.448704
9.245752	555.998091	10.453722
8.876651	538.971373	10.458739
8.932793	533.321733	10.463757
8.779262	540.160368	10.468775
8.688551	553.548889	10.473792
9.114763	560.594028	10.478810
9.199778	562.862686	10.483827
9.216451	554.507616	10.488845
9.221340	542.003091	10.493863
8.910983	535.152072	10.498880
8.957030	527.258602	10.503898
8.621159	537.061899	10.508915
8.997013	548.332297	10.513933
8.856287	548.843550	10.518951
9.057618	551.233507	10.523968
9.079964	551.824580	10.528986
8.770648	559.024431	10.534003
9.049664	558.836822	10.539021
8.754648	557.445621	10.544039
8.849313	552.427272	10.549056
9.094852	554.807168	10.554074
8.531271	572.216249	10.559091
9.067026	552.968753	10.564109
9.173515	554.911389	10.569127
9.248100	558.631177	10.574144
9.222088	557.547320	10.579162
8.950879	564.094158	10.584179
8.935065	548.195419	10.589197
8.774468	557.448119	10.594215
8.822969	567.203069	10.599232
9.122680	569.784209	10.604250
8.995770	595.604755	10.609267
9.507728	592.325136	10.614285
9.082424	589.973970	10.619303
8.958973	589.506583	10.624320
9.563693	583.447829	10.629338
9.274110	590.405899	10.634355
8.958833	581.442913	10.639373
9.005694	586.029712	10.644391
9.415319	592.055275	10.649408
9.583182	575.633636	10.654426
9.463362	586.245674	10.659443
9.573214	585.963309	10.664461
9.276554	563.460942	10.669479
9.128001	564.351758	10.674496
9.207334	567.894225	10.679514
9.249020	576.812979	10.684531
9.521199	574.230926	10.689549
9.708537	588.255475	10.694567
9.241920	563.349013	10.699584
9.087071	549.859669	10.704602
9.199560	575.559435	10.709619
9.651238	582.929344	10.714637
9.436237	562.034021	10.719655
8.912218	572.117889	10.724672
9.613695	573.813314	10.729690
9.174625	586.897794	10.734707
9.672469	579.171318	10.739725
9.803632	578.490728	10.744743
9.244297	565.225565	10.749760
9.327463	560.089649	10.754778
9.198615	567.798940	10.759795
9.573546	578.235924	10.764813
9.783775	585.642389	10.769831
9.758697	572.938502	10.774848
9.616911	552.093679	10.779866
9.281016	554.914078	10.784883
9.534000	550.480169	10.789901
9.243862	552.857958	10.794919
9.318799	546.796728	10.799936
9.214377	566.608547	10.804954
9.539264	577.926457	10.809971
9.543698	577.910773	10.814989
9.852712	575.965611	10.820007
9.617979	576.995250	10.825024
9.802695	562.144928	10.830042
9.219520	561.082392	10.835059
9.298140	566.980596	10.840077
9.748520	577.272757	10.845095
9.262239	592.365324	10.850112
9.302953	595.742069	10.855130
9.610648	601.853856	10.860147
9.510149	590.846722	10.865165
9.390633	593.982677	10.870183
9.421405	593.288467	10.875200
9.779663	596.778352	10.880218
9.574992	597.545498	10.885235
9.459048	588.253170	10.890253
9.336035	592.542224	10.895271
9.321279	588.434776	10.900288
9.651531	578.229026	10.905306
9.707597	588.960591	10.910323
9.714755	597.574300	10.915341
9.753243	588.058361	10.920359
9.548655	593.483208	10.925376
9.828873	607.104315	10.930394
9.800509	609.901752	10.935411
9.623460	605.492347	10.940429
9.951341	615.463901	10.945447
9.682589	616.053683	10.950464
10.009615	604.039758	10.955482
10.018155	614.066741	10.960499
10.049294	590.810403	10.965517
9.944654	591.180189	10.970535
9.751668	602.625325	10.975552
9.869050	587.744480	10.980570
9.741369	584.117018	10.985587
10.019343	590.933373	10.990605
9.886079	588.429243	10.995623
9.598689	586.961499	11.000640
9.928165	590.051005	11.005658
9.831712	586.307676	11.010675
9.768870	587.767576	11.015693
9.764406	585.607146	11.020711
9.928248	601.109404	11.025728
10.005318	594.686064	11.030746
9.937451	593.235378	11.035763
10.247630	602.921128	11.040781
9.932056	607.799868	11.045799
9.644571	591.805358	11.050816
10.069361	597.180222	11.055834
10.068688	590.552847	11.060851
9.834439	600.415359	11.065869
10.009253	595.466410	11.070887
9.823908	598.522122	11.075904
10.047996	594.818320	11.080922
10.052843	615.224619	11.085939
10.297812	620.066624	11.090957
10.242691	589.097951	11.095975
10.133849	596.790075	11.100992
10.073619	584.406884	11.106010
9.766537	586.304604	11.111027
10.033252	588.812574	11.116045
9.927523	589.875313	11.121063
9.782725	605.166626	11.126080
10.365997	617.258727	11.131098
10.325382	611.510602	11.136115
9.997261	601.274689	11.141133
10.572929	607.030544	11.146151
9.888871	599.358458	11.151168
10.034848	587.714555	11.156186
9.975934	594.383869	11.161203
10.245441	622.002745	11.166221
10.430641	613.437644	11.171239
10.176437	621.961809	11.176256
10.191115	615.035686	11.181274
9.940446	602.576887	11.186291
9.885624	611.976279	11.191309
10.168620	609.909258	11.196327
10.009841	623.102634	11.201344
10.229575	620.891568	11.206362
9.813305	615.374877	11.211379
9.983977	627.544815	11.216397
9.992169	617.689052	11.221415
10.072100	619.688240	11.226432
9.585644	627.709362	11.231450
10.267685	631.111306	11.236467
10.233370	646.752537	11.241485
10.624659	631.771376	11.246503
10.312588	650.476016	11.251520
10.603603	641.042993	11.256538
10.509870	651.355549	11.261555
10.450828	631.748958	11.266573
10.755102	616.897227	11.271591
10.425989	624.109040	11.276608
10.123217	619.477248	11.281626
10.391430	610.148188	11.286643
10.428159	619.563257	11.291661
10.252909	604.771692	11.296679
9.975597	619.605979	11.301696
10.728759	629.422829	11.306714
10.845510	640.693899	11.311731
10.444963	626.340350	11.316749
10.655190	621.951274	11.321767
10.327507	616.792505	11.326784
10.565910	623.291365	11.331802
10.303865	614.991966	11.336819
10.236127	623.551052	11.341837
10.529186	630.793488	11.346855
10.549449	638.685906	11.351872
10.616596	646.341788	11.356890
10.673231	647.601474	11.361907
10.826073	636.717664	11.366925
10.857755	631.455713	11.371943
10.408514	632.199706	11.376960
10.424584	621.570255	11.381978
10.407498	615.252901	11.386995
10.596829	644.758508	11.392013
10.781837	654.981704	11.397031
10.781778	650.611429	11.402048
10.779935	635.549789	11.407066
10.529482	622.762755	11.412083
10.268831	622.876786	11.417101
10.613536	631.596018	11.422119
10.460582	656.373444	11.427136
10.630570	644.067590	11.432154
10.725460	647.959698	11.437171
10.527062	648.148858	11.442189
10.697758	641.148918	11.447207
10.716829	646.702439	11.452224
10.662393	651.370158	11.457242
10.913361	646.167417	11.462259
10.976302	647.757883	11.467277
10.531909	639.243772	11.472295
10.631080	648.766036	11.477312
10.657887	644.192741	11.482330
10.645231	649.660776	11.487347
10.441084	646.760852	11.492365
10.750948	644.488048	11.497383
10.668215	646.744193	11.502400
10.519724	641.160114	11.507418
10.937599	651.914298	11.512435
10.586195	643.467774	11.517453
10.694108	651.226152	11.522471
10.522678	658.392634	11.527488
10.884060	670.866260	11.532506
11.079189	676.279794	11.537523
10.746887	677.479863	11.542541
11.041613	677.414140	11.547559
10.871595	679.570268	11.552576
10.781250	679.964952	11.557594
11.274452	681.192546	11.562611
11.200464	689.653706	11.567629
11.054327	654.031374	11.572647
10.899184	658.206784	11.577664
11.104567	650.952633	11.582682
11.193523	640.235548	11.587699
10.635964	648.190494	11.592717
10.765639	654.231249	11.597735
11.166653	666.613792	11.602752
11.191249	681.334873	11.607770
10.997265	676.749443	11.612787
11.124144	676.821869	11.617805
11.495461	678.708849	11.622823
11.353518	674.045148	11.627840
11.104473	652.745270	11.632858
11.180402	651.878962	11.637875
10.893633	658.078777	11.642893
11.173730	647.010970	11.647911
10.936238	653.491853	11.652928
10.841629	655.884088	11.657946
11.258660	664.727974	11.662963
11.004774	685.205463	11.667981
11.152195	685.726079	11.672999
11.136234	684.720654	11.678016
10.886309	689.948441	11.683034
11.340538	676.556324	11.688051
10.560360	695.241643	11.693069
10.817135	689.850858	11.698087
10.984462	683.491291	11.703104
11.047368	678.437212	11.708122
11.257799	690.325094	11.713139
11.263129	687.038842	11.718157
11.269377	687.782748	11.723175
11.095855	684.723850	11.728192
11.086715	693.475712	11.733210
11.393666	694.659593	11.738227
11.411966	712.862557	11.743245
11.344903	704.770604	11.748263
11.544440	705.739015	11.753280
11.522902	690.858099	11.758298
11.824650	684.938726	11.763315
11.412312	682.068773	11.768333
11.380460	688.238281	11.773351
11.252180	688.704674	11.778368
11.245668	685.820105	11.783386
11.217333	680.601611	11.788403
11.159179	691.540571	11.793421
11.230799	680.939588	11.798439
11.577501	708.003842	11.803456
11.369320	719.825813	11.808474
11.822744	712.119306	11.813491
11.393887	697.920930	11.818509
11.566206	691.972166	11.823527
11.912711	695.736305	11.828544
11.550702	694.424850	11.833562
11.588909	673.854585	11.838579
11.250300	687.797965	11.843597
11.224574	686.918342	11.848615
11.540707	688.861776	11.853632
11.548402	697.937664	11.858650
11.745213	710.050996	11.863667
11.656033	704.216983	11.868685
11.562437	693.910958	11.873703
11.769831	698.920091	11.878720
11.288405	692.934213	11.883738
11.525258	707.524395	11.888755
11.846571	725.538645	11.893773
11.882362	713.094117	11.898791
11.852752	701.514177	11.903808
11.599133	697.348161	11.908826
11.618097	679.782644	11.913843
11.355090	693.670041	11.918861
11.550821	715.392005	11.923879
11.718158	714.121195	11.928896
11.599970	717.475319	11.933914
11.893415	717.439920	11.938931
11.452769	723.973692	11.943949
12.237256	721.100694	11.948967
12.130992	725.841653	11.953984
11.674838	734.185220	11.959002
12.291361	719.825287	11.964019
11.878039	711.429304	11.969037
11.578571	695.088013	11.974055
11.850124	693.141254	11.979072
11.897810	702.538228	11.984090
11.778467	687.231144	11.989107
11.678457	695.892238	11.994125
11.940613	709.776705	11.999143
12.229094	697.808735	12.004160
11.904134	705.101969	12.009178
11.563632	695.761663	12.014195
11.908089	704.223843	12.019213
11.895221	716.391709	12.024231
12.215430	721.409563	12.029248
11.976218	721.565908	12.034266
11.951255	713.469848	12.039283
12.085714	710.349322	12.044301
11.940406	710.783498	12.049319
11.933451	722.603215	12.054336
11.752554	718.597976	12.059354
11.669788	719.308769	12.064371
11.892003	724.824909	12.069389
11.979100	712.777926	12.074407
11.979054	714.447693	12.079424
11.779243	721.241508	12.084442
11.957531	717.728675	12.089459
11.923073	718.917413	12.094477
11.743599	717.857921	12.099495
11.949573	712.262474	12.104512
11.699006	718.142907	12.109530
12.145011	728.696078	12.114547
12.502402	730.956553	12.119565
12.168966	731.638115	12.124583
12.079076	709.019491	12.129600
11.962720	716.613724	12.134618
12.435857	732.940225	12.139635
12.344350	721.699372	12.144653
12.005938	726.413550	12.149671
12.424531	723.646678	12.154688
12.333660	721.011528	12.159706
12.610952	716.109964	12.164723
12.187626	719.361394	12.169741
12.157931	702.488897	12.174759
12.037039	703.880266	12.179776
11.929538	716.874341	12.184794
12.266341	731.512878	12.189811
12.210393	742.935668	12.194829
12.109625	740.944841	12.199847
12.623634	741.906651	12.204864
11.976550	744.535742	12.209882
12.132092	740.725638	12.214899
12.171718	739.055048	12.219917
11.624529	745.963159	12.224935
11.842886	742.653501	12.229952
12.010593	744.010269	12.234970
12.468937	760.425251	12.239987
12.816175	769.460619	12.245005
12.700395	763.743850	12.250023
12.566515	747.818952	12.255040
12.544196	746.559111	12.260058
12.450439	740.642589	12.265075
12.446849	744.492937	12.270093
12.411023	747.115977	12.275111
12.696080	739.059991	12.280128
12.611004	742.632915	12.285146
12.434220	738.455962	12.290163
12.522033	743.184437	12.295181
12.256615	736.164810	12.300199
12.911133	760.234567	12.305216
12.737054	759.930138	12.310234
12.343254	748.423336	12.315251
12.842356	757.302326	12.320269
12.577301	766.315868	12.325287
12.971303	746.593030	12.330304
12.676399	745.659579	12.335322
12.855158	748.769990	12.340339
12.710914	742.807588	12.345357
12.458445	739.768023	12.350375
12.726361	740.462686	12.355392
12.855314	750.469958	12.360410
12.624155	738.104065	12.365427
12.851997	737.008061	12.370445
12.458074	741.952241	12.375463
12.901719	736.948096	12.380480
12.661619	756.308460	12.385498
12.691432	739.207528	12.390515
12.932713	744.221605	12.395533
12.727739	757.559220	12.400551
12.820614	746.645880	12.405568
12.261861	750.343138	12.410586
12.623580	768.370246	12.415603
13.032613	766.376845	12.420621
13.405082	767.482595	12.425639
13.316351	769.576197	12.430656
13.067861	754.446855	12.435674
12.992282	747.776585	12.440691
13.227542	750.113337	12.445709
12.663489	743.979609	12.450727
13.040235	739.240407	12.455744
12.888348	750.917889	12.460762
12.609754	742.812752	12.465779
13.142884	730.431565	12.470797
12.943917	739.771211	12.475815
13.214983	724.531929	12.480832
13.101333	736.316937	12.485850
12.910576	740.233935	12.490867
12.966559	733.552164	12.495885
12.736127	731.884479	12.500903
12.979938	743.908099	12.505920
12.954805	748.507434	12.510938
13.214611	769.782259	12.515955
13.470650	768.063405	12.520973
12.860502	747.255763	12.525991
13.041224	744.202669	12.531008
13.349995	770.062315	12.536026
12.989080	758.797956	12.541043
13.077767	747.531931	12.546061
13.154721	769.671064	12.551079
13.260355	775.144689	12.556096
13.511471	762.068293	12.561114
13.115834	753.980426	12.566131
13.269189	755.718136	12.571149
12.937214	756.734826	12.576167
13.357186	756.027265	12.581184
13.082432	765.384175	12.586202
13.076503	775.967485	12.591219
13.235411	766.739154	12.596237
13.125143	773.400796	12.601255
13.413501	776.929730	12.606272
13.278521	773.194690	12.611290
13.298847	778.441220	12.616307
13.236730	772.103886	12.621325
12.907824	779.314949	12.626343
13.245422	765.961218	12.631360
13.269870	771.660324	12.636378
13.409979	764.444953	12.641395
13.472433	772.196832	12.646413
13.216812	780.309685	12.651431
13.152989	776.556489	12.656448
13.582334	768.665682	12.661466
13.468242	774.422716	12.666483
13.464308	768.269728	12.671501
13.258974	773.861658	12.676519
13.444041	767.096249	12.681536
13.547003	776.618556	12.686554
13.495890	792.835239	12.691571
13.646243	779.029954	12.696589
13.502526	783.748484	12.701607
13.429955	801.223502	12.706624
13.523560	790.798501	12.711642
13.654435	805.547699	12.716659
13.790448	794.015600	12.721677
13.757949	791.915570	12.726695
13.635337	783.154440	12.731712
13.835532	776.113252	12.736730
13.328894	780.891756	12.741747
13.577399	779.106836	12.746765
13.644475	801.222848	12.751783
13.725010	804.222853	12.756800
14.120602	789.111719	12.761818
13.846441	782.898087	12.766835
13.885148	774.964569	12.771853
13.655183	763.659082	12.776871
13.546666	763.520064	12.781888
13.782931	772.309354	12.786906
13.784359	790.560859	12.791923
13.935905	781.008503	12.796941
13.521687	789.270183	12.801959
13.439259	793.614976	12.806976
13.562740	789.588744	12.811994
13.812678	798.708994	12.817011
13.912092	796.066987	12.822029
13.920708	799.921335	12.827047
13.752277	791.057852	12.832064
13.831500	797.002493	12.837082
13.940105	811.051180	12.842099
13.995527	790.867505	12.847117
14.088747	789.956213	12.852135
13.864502	805.064532	12.857152
14.235328	791.440181	12.862170
13.776915	791.398938	12.867187
14.168363	794.047421	12.872205
14.189280	798.718182	12.877223
14.025968	793.260588	12.882240
14.189984	801.169680	12.887258
13.989485	798.795698	12.892275
13.997398	787.768835	12.897293
14.067703	787.772771	12.902311
14.108268	801.262428	12.907328
14.224951	797.650034	12.912346
14.070226	802.782024	12.917363
14.299158	801.314646	12.922381
14.017265	799.159981	12.927399
14.127667	797.730593	12.932416
13.990043	797.999654	12.937434
13.902471	801.208212	12.942451
14.039929	796.417215	12.947469
14.003654	802.908699	12.952487
14.069433	792.227418	12.957504
14.290274	789.304471	12.962522
13.782425	792.727728	12.967539
14.062956	796.635841	12.972557
14.040960	810.833055	12.977575
14.379271	837.863498	12.982592
14.773161	822.781446	12.987610
14.662914	811.230690	12.992627
14.596421	803.868572	12.997645
14.510898	791.534168	13.002663
14.033439	796.747732	13.007680
14.317338	794.596990	13.012698
14.247384	793.754388	13.017715
14.249993	787.575513	13.022733
14.376269	791.434327	13.027751
14.341225	794.465435	13.032768
14.244353	800.282318	13.037786
14.135983	821.288789	13.042803
14.516863	829.426969	13.047821
14.510034	829.573845	13.052839
14.608044	825.233270	13.057856
14.777559	828.957905	13.062874
14.410436	831.558557	13.067891
14.245210	823.261053	13.072909
14.622602	837.321831	13.077927
14.813549	830.261187	13.082944
14.638711	821.535629	13.087962
14.622487	828.901401	13.092979
14.628952	828.678629	13.097997
14.714982	818.889091	13.103015
14.601028	838.788548	13.108032
14.720815	824.094542	13.113050
14.216217	833.752813	13.118067
14.320624	829.604450	13.123085
14.490733	836.895151	13.128103
14.611790	836.222813	13.133120
14.804875	829.112908	13.138138
14.460378	827.410529	13.143155
14.658268	829.602612	13.148173
14.654834	833.855539	13.153191
14.711683	830.645176	13.158208
14.927029	829.352351	13.163226
14.828703	831.951291	13.168243
14.498711	830.277021	13.173261
14.570400	825.632487	13.178279
14.308911	837.531652	13.183296
14.984269	843.752038	13.188314
14.879151	848.667813	13.193331
14.957580	853.264531	13.198349
15.113337	851.046195	13.203367
14.826447	846.256127	13.208384
15.047912	843.345958	13.213402
15.083073	858.965984	13.218419
15.074773	846.669651	13.223437
14.812287	843.176392	13.228455
14.834226	855.545860	13.233472
15.201562	846.574815	13.238490
14.942669	851.350187	13.243507
15.109338	866.722152	13.248525
14.952377	859.295740	13.253543
14.661455	862.846617	13.258560
15.213073	864.881253	13.263578
14.926335	864.006276	13.268595
14.920162	852.315971	13.273613
15.053293	854.400770	13.278631
15.069758	854.015548	13.283648
15.151484	846.600672	13.288666
14.968727	852.745095	13.293683
14.905607	857.173805	13.298701
14.913653	863.485975	13.303719
14.912330	855.290774	13.308736
15.273828	855.164715	13.313754
15.220785	866.012715	13.318771
15.300265	844.780698	13.323789
15.515279	842.714942	13.328807
15.055907	860.706030	13.333824
15.165016	853.580074	13.338842
15.218969	849.976067	13.343859
14.852600	852.708758	13.348877
15.435262	868.621512	13.353895
15.355865	882.404538	13.358912
15.760812	880.233386	13.363930
15.482826	875.346482	13.368947
15.357970	858.183297	13.373965
15.644372	853.200278	13.378983
15.212408	859.322906	13.384000
15.320080	862.347763	13.389018
15.357286	865.301111	13.394035
15.217777	885.009611	13.399053
15.760194	878.343830	13.404071
15.649248	894.002995	13.409088
15.724088	886.497128	13.414106
15.510602	879.559880	13.419123
15.303324	873.104197	13.424141
15.796804	887.005803	13.429159
15.546410	881.452943	13.434176
16.021242	866.203367	13.439194
15.740146	865.389159	13.444211
15.355314	856.549000	13.449229
15.833997	846.944608	13.454247
15.355756	862.269531	13.459264
15.502808	862.396291	13.464282
15.695290	869.596417	13.469299
15.703991	884.163655	13.474317
15.846140	880.240692	13.479335
15.863795	873.269284	13.484352
15.687384	851.617721	13.489370
15.486633	869.714676	13.494387
15.688976	878.237931	13.499405
15.876824	879.702583	13.504423
15.690001	882.756626	13.509440
15.818210	883.050152	13.514458
16.130503	882.850743	13.519475
15.504759	876.408907	13.524493
15.801489	879.379497	13.529511
15.707732	888.767485	13.534528
15.884167	881.372170	13.539546
16.098887	884.855829	13.544563
15.868960	887.839845	13.549581
16.080706	873.823578	13.554599
15.957605	885.893379	13.559616
15.921151	881.812269	13.564634
15.937294	884.148744	13.569651
15.783523	877.626747	13.574669
16.215350	879.699287	13.579687
16.059924	895.777638	13.584704
16.243970	886.417545	13.589722
16.170672	888.726191	13.594739
15.887343	890.977142	13.599757
16.350897	878.146395	13.604775
16.211567	887.695428	13.609792
16.142921	878.810386	13.614810
16.177847	873.737741	13.619827
15.970579	884.486461	13.624845
16.195146	877.516874	13.629863
16.200581	881.406702	13.634880
15.817045	875.703339	13.639898
16.017165	879.303561	13.644915
15.966041	890.114358	13.649933
16.308421	877.179152	13.654951
15.744275	890.943590	13.659968
15.938556	882.021492	13.664986
16.108148	884.993708	13.670003
15.740180	890.467307	13.675021
16.237960	903.596116	13.680039
16.455326	916.148358	13.685056
16.027105	911.173691	13.690074
16.562221	907.282024	13.695091
16.340464	920.529066	13.700109
16.738711	905.549344	13.705127
16.563065	915.268735	13.710144
16.727057	905.677539	13.715162
16.556188	895.401271	13.720179
16.489414	889.738059	13.725197
16.511300	883.692056	13.730215
16.282079	883.053788	13.735232
16.380559	896.499810	13.740250
16.652716	900.344286	13.745267
16.445979	904.547675	13.750285
16.618783	908.076841	13.755303
16.624480	915.397308	13.760320
16.733105	903.265826	13.765338
16.580301	903.889990	13.770355
16.624189	915.853493	13.775373
16.969127	897.768490	13.780391
16.508379	886.901764	13.785408
16.419193	892.554450	13.790426
16.796207	894.119217	13.795443
16.391669	896.315114	13.800461
16.381543	896.674307	13.805479
16.668634	905.639689	13.810496
16.581601	902.288158	13.815514
16.560941	898.833944	13.820531
16.375244	914.212819	13.825549
16.687016	907.150771	13.830567
16.527616	902.779498	13.835584
16.467452	905.279740	13.840602
16.581671	904.765981	13.845619
16.722043	921.395957	13.850637
17.259561	921.839618	13.855655
16.999645	912.213371	13.860672
17.043566	902.760797	13.865690
17.092987	894.222703	13.870707
16.771491	891.470349	13.875725
17.097068	895.385313	13.880743
16.988686	901.736125	13.885760
16.999511	904.475770	13.890778
17.047187	899.220728	13.895795
17.005434	904.124278	13.900813
16.982314	907.586135	13.905831
17.373586	901.582607	13.910848
16.659976	893.996933	13.915866
17.079932	895.240586	13.920883
16.995985	901.883960	13.925901
17.167150	908.215739	13.930919
17.089843	915.003269	13.935936
17.110317	926.086460	13.940954
17.172154	922.336474	13.945971
17.188842	930.863475	13.950989
17.436674	926.917328	13.956007
17.324966	924.594783	13.961024
17.525350	920.461927	13.966042
17.356042	896.975897	13.971059
17.234708	902.220589	13.976077
16.950063	902.315263	13.981095
17.316314	901.692545	13.986112
17.381126	909.062973	13.991130
17.434984	907.516564	13.996147
17.068929	908.172722	14.001165
17.298771	925.105378	14.006183
17.298027	931.978672	14.011200
17.381095	919.980018	14.016218
17.386266	928.417403	14.021235
17.489675	934.076852	14.026253
17.754258	924.524424	14.031271
17.468356	927.480008	14.036288
17.534897	927.766504	14.041306
17.564266	914.208411	14.046323
17.372884	920.979271	14.051341
17.544495	926.953864	14.056359
17.888273	924.342798	14.061376
17.753326	912.898785	14.066394
17.549449	901.603646	14.071411
17.456716	913.586183	14.076429
17.503560	918.520462	14.081447
17.816276	923.106924	14.086464
17.749673	928.985180	14.091482
17.865037	922.591097	14.096499
17.587791	916.259438	14.101517
17.754597	914.524906	14.106535
18.007986	913.641460	14.111552
17.434827	910.118044	14.116570
17.660590	909.311394	14.121587
17.612971	906.838227	14.126605
17.920993	916.624318	14.131623
18.203128	920.664162	14.136640
17.701760	919.352196	14.141658
17.841289	911.426253	14.146675
17.549342	921.628169	14.151693
18.047668	918.947971	14.156711
17.843323	926.221475	14.161728
17.742367	930.889094	14.166746
17.827736	912.533737	14.171763
18.227043	920.512356	14.176781
18.086008	928.497019	14.181799
18.031282	923.714911	14.186816
18.100067	929.531431	14.191834
18.088486	914.872628	14.196851
17.665855	917.369594	14.201869
17.744305	925.444045	14.206887
17.820386	915.740917	14.211904
17.530566	921.761845	14.216922
17.626489	913.887686	14.221939
17.711268	921.623847	14.226957
17.999576	912.802313	14.231975
18.101650	922.079824	14.236992
18.092201	944.055566	14.242010
18.567011	940.012370	14.247027
18.216766	926.597398	14.252045
18.147659	935.312072	14.257063
18.142304	918.554486	14.262080
17.986252	928.244078	14.267098
18.228660	948.145700	14.272115
18.220570	938.402048	14.277133
18.234423	948.354073	14.282151
18.176899	946.855295	14.287168
18.118007	944.877104	14.292186
18.364303	942.621552	14.297203
18.504393	946.285834	14.302221
18.393447	940.893143	14.307239
18.688997	937.684937	14.312256
18.277244	939.325047	14.317274
18.750132	932.453843	14.322291
18.172537	942.345266	14.327309
18.329402	938.452627	14.332327
18.751213	941.675344	14.337344
18.355735	937.154624	14.342362
18.679709	934.891944	14.347379
18.517843	932.659168	14.352397
18.482393	944.915675	14.357415
18.420458	929.049553	14.362432
18.220985	936.914571	14.367450
18.557025	930.403126	14.372467
18.755609	936.016145	14.377485
18.505761	941.430486	14.382503
18.579742	939.055110	14.387520
18.740954	940.058211	14.392538
18.510885	936.872804	14.397555
18.632245	941.805503	14.402573
18.824852	948.820245	14.407591
19.203335	944.340391	14.412608
18.753669	947.929625	14.417626
18.749835	928.547643	14.422643
18.590928	940.010326	14.427661
18.474093	950.557468	14.432679
18.956053	956.093749	14.437696
18.801563	969.474770	14.442714
19.025842	972.514625	14.447731
19.025754	970.420826	14.452749
18.873265	976.623474	14.457767
19.621677	970.254164	14.462784
19.164270	943.311377	14.467802
19.193026	936.424901	14.472819
19.209923	928.050697	14.477837
18.885482	937.409525	14.482855
19.249129	936.271974	14.487872
19.156868	934.780413	14.492890
19.417351	928.893549	14.497907
19.137161	931.800463	14.502925
19.212935	938.191120	14.507943
19.675811	918.587464	14.512960
19.282162	925.802406	14.517978
19.337592	924.746493	14.522995
19.201196	915.494938	14.528013
18.885027	935.601528	14.533031
19.162478	933.346438	14.538048
19.119929	934.671545	14.543066
18.992805	932.740353	14.548083
19.165800	926.416455	14.553101
18.748290	931.992924	14.558119
19.175695	933.760255	14.563136
19.167578	929.798442	14.568154
18.888258	923.415655	14.573171
19.314989	948.527993	14.578189
18.965571	953.630603	14.583207
19.326608	964.740697	14.588224
19.511387	957.943565	14.593242
19.025488	959.500178	14.598259
19.199955	966.254490	14.603277
19.008492	967.402866	14.608295
20.037443	961.592012	14.613312
19.920977	965.996406	14.618330
19.665952	957.404669	14.623347
19.748507	960.856849	14.628365
19.711763	969.812607	14.633383
19.883903	952.982057	14.638400
19.348105	952.641353	14.643418
19.353456	958.253543	14.648435
19.550623	967.290800	14.653453
19.583444	955.999608	14.658471
19.744122	961.320824	14.663488
19.625065	961.518328	14.668506
19.641685	960.261777	14.673523
20.019219	960.092523	14.678541
19.677857	956.814205	14.683559
19.485395	947.835627	14.688576
19.216955	964.514511	14.693594
19.501009	973.145357	14.698611
19.920642	977.282059	14.703629
19.067412	991.141594	14.708647
19.809742	986.493352	14.713664
19.838011	990.391932	14.718682
19.712345	994.543174	14.723699
20.107718	995.730673	14.728717
20.116180	990.727903	14.733735
20.012740	996.446357	14.738752
20.076763	990.184232	14.743770
19.782774	989.279841	14.748787
20.136888	985.846533	14.753805
19.935404	982.403583	14.758823
19.925472	980.552805	14.763840
20.086312	991.849714	14.768858
20.189319	975.635378	14.773875
20.327892	980.323851	14.778893
20.189664	982.937185	14.783911
20.423164	987.318588	14.788928
20.073722	987.350460	14.793946
20.495210	991.868387	14.798963
20.639583	985.855833	14.803981
20.389444	987.880289	14.808999
20.263947	986.193955	14.814016
20.325335	992.534758	14.819034
20.162318	989.173131	14.824051
20.158538	990.440172	14.829069
20.081832	990.256432	14.834087
20.228299	986.652161	14.839104
20.057301	990.120268	14.844122
20.061428	990.888649	14.849139
20.468384	1003.391132	14.854157
20.518066	1012.160123	14.859175
20.990017	1015.966888	14.864192
20.966438	989.665392	14.869210
20.408466	985.759692	14.874227
20.369141	987.622266	14.879245
20.659334	985.041105	14.884263
20.769335	974.655387	14.889280
20.534827	980.264416	14.894298
20.462200	978.364461	14.899315
20.641154	976.408072	14.904333
20.309197	977.217330	14.909351
20.854780	972.635358	14.914368
20.899089	971.047124	14.919386
20.695057	973.854861	14.924403
20.826435	969.033914	14.929421
20.741663	981.390022	14.934439
20.938504	977.050195	14.939456
20.581594	973.566212	14.944474
20.396918	971.764780	14.949491
21.163863	988.992341	14.954509
20.801090	991.202212	14.959527
20.656169	999.172006	14.964544
20.661812	1001.631571	14.969562
20.836805	1006.792394	14.974579
21.130222	1005.227841	14.979597
21.205002	1020.460744	14.984615
21.171042	1013.077698	14.989632
21.292970	1005.193782	14.994650
20.411295	993.091849	14.999667
21.527659	997.253945	15.004685
20.935175	999.391758	15.009703
21.313639	1002.602659	15.014720
21.181978	992.074614	15.019738
20.921127	984.016212	15.024755
21.163553	984.282795	15.029773
20.960577	1008.133590	15.034791
21.280429	1011.326428	15.039808
21.088196	1016.668195	15.044826
20.955376	1021.292788	15.049843
21.397914	1006.676549	15.054861
20.764128	1024.192802	15.059879
20.925979	1016.734490	15.064896
21.475807	1007.637442	15.069914
21.296767	1019.939880	15.074931
21.305421	1006.992699	15.079949
21.420016	1006.870440	15.084967
21.278192	1014.451708	15.089984
20.932567	1012.367573	15.095002
20.932873	1006.008215	15.100019
21.427036	1005.822738	15.105037
21.209725	1026.199181	15.110055
21.332734	1030.709466	15.115072
21.726739	1033.338183	15.120090
21.604326	1042.924175	15.125107
21.673499	1028.699085	15.130125
22.006037	1033.244812	15.135143
21.610410	1022.559615	15.140160
21.421396	1010.106827	15.145178
21.643970	1017.966894	15.150195
22.006621	1023.132630	15.155213
21.586855	1025.101475	15.160231
21.471872	1011.629050	15.165248
22.019861	1017.918579	15.170266
22.070456	1019.085216	15.175283
21.866021	1005.438930	15.180301
21.539317	1003.388080	15.185319
21.912246	1002.070479	15.190336
21.894318	997.026210	15.195354
21.857418	999.040621	15.200371
21.930295	989.411093	15.205389
21.765634	1002.411017	15.210407
21.609621	1004.859409	15.215424
21.804296	1004.281475	15.220442
21.444809	1029.577209	15.225459
22.028255	1040.508699	15.230477
22.114177	1035.511319	15.235495
21.943296	1014.400939	15.240512
22.243882	1019.359056	15.245530
22.216338	1030.958633	15.250547
22.400439	1025.032986	15.255565
22.221591	1025.242733	15.260583
22.029399	1035.145907	15.265600
22.211808	1023.332887	15.270618
22.321169	1026.516426	15.275635
22.036299	1026.780203	15.280653
21.878939	1031.110187	15.285671
22.115317	1040.543004	15.290688
22.296709	1031.067633	15.295706
21.857372	1027.764060	15.300723
22.100701	1029.854290	15.305741
22.040106	1021.682867	15.310759
21.952720	1031.300459	15.315776
22.057751	1030.360533	15.320794
21.649868	1044.942937	15.325811
22.055408	1044.128320	15.330829
22.378726	1059.135576	15.335847
22.648430	1058.739498	15.340864
22.595924	1061.115489	15.345882
22.703745	1063.124986	15.350899
22.399370	1069.818242	15.355917
22.728677	1056.457069	15.360935
22.525390	1061.960591	15.365952
22.856297	1068.660458	15.370970
22.508616	1055.651474	15.375987
22.736689	1052.313377	15.381005
22.908713	1047.783669	15.386023
22.868988	1055.352907	15.391040
22.726965	1043.301114	15.396058
22.635944	1050.133582	15.401075
23.127145	1048.224878	15.406093
23.017399	1026.179441	15.411111
22.632311	1029.023111	15.416128
22.915197	1020.615430	15.421146
22.704386	1030.183351	15.426163
22.973913	1012.194716	15.431181
22.838313	1012.736430	15.436199
22.647320	1018.908260	15.441216
22.710807	1034.031054	15.446234
22.938721	1046.401771	15.451251
22.992645	1061.819921	15.456269
22.700838	1055.051119	15.461287
22.872051	1049.519159	15.466304
23.142979	1050.457392	15.471322
22.987133	1050.897353	15.476339
22.935335	1048.375157	15.481357
22.983528	1049.035292	15.486375
22.943671	1054.413101	15.491392
23.132684	1048.701065	15.496410
23.197554	1047.695937	15.501427
22.857018	1048.100190	15.506445
23.149100	1054.622739	15.511463
22.974686	1057.521348	15.516480
23.227179	1042.220561	15.521498
22.828719	1046.028383	15.526515
22.850321	1050.459975	15.531533
23.116502	1065.928374	15.536551
23.053957	1077.614957	15.541568
23.203398	1077.163077	15.546586
23.503816	1075.839346	15.551603
23.479756	1088.857932	15.556621
23.345316	1078.072851	15.561639
23.315234	1081.717264	15.566656
23.396389	1075.492030	15.571674
23.639465	1071.589047	15.576691
23.773053	1078.094892	15.581709
23.794087	1076.051910	15.586727
23.394626	1073.082033	15.591744
23.601787	1072.406873	15.596762
23.780487	1078.813448	15.601779
23.440380	1073.143771	15.606797
23.713992	1088.197452	15.611815
23.477765	1082.531862	15.616832
23.608431	1079.589811	15.621850
23.456259	1075.737972	15.626867
23.783813	1077.314376	15.631885
23.577229	1075.532593	15.636903
23.774282	1070.238538	15.641920
23.639311	1070.303853	15.646938
23.818422	1082.308220	15.651955
23.435982	1066.785815	15.656973
23.945809	1077.802123	15.661991
23.732035	1079.896258	15.667008
24.061314	1081.890416	15.672026
24.153347	1096.340952	15.677043
24.076896	1091.780061	15.682061
23.884842	1077.391142	15.687079
24.041320	1089.083265	15.692096
24.129583	1088.833391	15.697114
24.135850	1092.579262	15.702131
23.937558	1083.973847	15.707149
24.293406	1099.134401	15.712167
23.974502	1105.510345	15.717184
23.963439	1103.939710	15.722202
24.319861	1096.543383	15.727219
24.163420	1096.288286	15.732237
24.260005	1101.131249	15.737255
24.352642	1105.576705	15.742272
24.375756	1101.657316	15.747290
24.266064	1112.378458	15.752307
24.252559	1098.559518	15.757325
24.367921	1097.916649	15.762343
24.427480	1105.437128	15.767360
24.322743	1105.779880	15.772378
24.215802	1100.373972	15.777395
24.517404	1113.366119	15.782413
24.714124	1100.763799	15.787431
24.291062	1106.758992	15.792448
24.565723	1104.279672	15.797466
24.226784	1097.156300	15.802483
24.386052	1099.677683	15.807501
24.525651	1100.903129	15.812519
24.027477	1101.582111	15.817536
24.320578	1101.459777	15.822554
24.216353	1108.842391	15.827571
24.490963	1114.252491	15.832589
24.869639	1120.821575	15.837607
24.650980	1130.794921	15.842624
24.910502	1118.719717	15.847642
25.088408	1124.578406	15.852659
24.880905	1128.173029	15.857677
25.203970	1120.128769	15.862695
25.360096	1114.016700	15.867712
25.055050	1095.724856	15.872730
25.079659	1092.890471	15.877747
24.902519	1092.261103	15.882765
25.090025	1080.065962	15.887783
24.914861	1085.693072	15.892800
24.631963	1081.686486	15.897818
24.823366	1074.429428	15.902835
24.739141	1095.840187	15.907853
25.291011	1088.291310	15.912871
24.975999	1101.367040	15.917888
25.083314	1107.814259	15.922906
25.174950	1117.763873	15.927923
25.219747	1121.816126	15.932941
25.398502	1115.543651	15.937959
25.021617	1118.869463	15.942976
25.130496	1120.554240	15.947994
25.174981	1116.467368	15.953011
25.083296	1117.925490	15.958029
25.022426	1111.604638	15.963047
25.062774	1118.571700	15.968064
25.460079	1116.850916	15.973082
25.404125	1113.605503	15.978099
25.373139	1125.316824	15.983117
25.505601	1109.130643	15.988135
25.168054	1117.120226	15.993152
25.275117	1121.077952	15.998170
25.618629	1116.660609	16.003187
25.263022	1115.653321	16.008205
25.297538	1106.418773	16.013223
25.207352	1131.120559	16.018240
25.182417	1141.317366	16.023258
25.659976	1136.328155	16.028275
25.563998	1143.333502	16.033293
26.042544	1139.879499	16.038311
25.899694	1144.067671	16.043328
26.023430	1141.421586	16.048346
26.173266	1139.098890	16.053363
25.884496	1129.953770	16.058381
26.062628	1123.351134	16.063399
25.592966	1110.165345	16.068416
25.803814	1119.216472	16.073434
25.862911	1130.148276	16.078451
25.768761	1132.150023	16.083469
26.218022	1129.532415	16.088487
26.032709	1138.575214	16.093504
25.893991	1141.924261	16.098522
26.040304	1141.590593	16.103539
25.889685	1143.834115	16.108557
26.219677	1139.810864	16.113575
25.960243	1154.310482	16.118592
25.713970	1141.853567	16.123610
26.012524	1132.358281	16.128627
25.959187	1134.078527	16.133645
26.044819	1145.471823	16.138663
26.224093	1147.345527	16.143680
26.125429	1138.326243	16.148698
26.240189	1138.915550	16.153715
26.113672	1144.987715	16.158733
26.289270	1133.134207	16.163751
26.206380	1145.823840	16.168768
26.494067	1136.847780	16.173786
26.714596	1136.175131	16.178803
26.112316	1147.865936	16.183821
26.219365	1133.188403	16.188839
26.252898	1141.071211	16.193856
26.066800	1162.307197	16.198874
26.367397	1163.271435	16.203891
26.393079	1172.207744	16.208909
26.468374	1167.686901	16.213927
26.399489	1164.259392	16.218944
26.449304	1168.683208	16.223962
26.736549	1159.739682	16.228979
26.614490	1167.668488	16.233997
26.984243	1152.998499	16.239015
27.159982	1160.069760	16.244032
27.066906	1174.000067	16.249050
27.234554	1152.505753	16.254067
26.710230	1161.217448	16.259085
26.752739	1170.651089	16.264103
27.176427	1159.899682	16.269120
27.058453	1160.999614	16.274138
27.366558	1159.203621	16.279155
27.035276	1151.155490	16.284173
27.014506	1137.022414	16.289191
26.970371	1133.570353	16.294208
26.893698	1135.564686	16.299226
26.913665	1134.501236	16.304243
26.884619	1156.507780	16.309261
27.125422	1153.823847	16.314279
27.256827	1161.089410	16.319296
27.118796	1161.959822	16.324314
27.222454	1153.377883	16.329331
27.104818	1155.402212	16.334349
27.074314	1153.463981	16.339367
27.110830	1149.332952	16.344384
26.905410	1150.087355	16.349402
26.909054	1146.007224	16.354419
26.821362	1150.342753	16.359437
27.096062	1154.188940	16.364455
27.513616	1171.230983	16.369472
27.426489	1190.180751	16.374490
27.654107	1177.812987	16.379507
27.380188	1184.594060	16.384525
27.506983	1186.245771	16.389543
27.779142	1185.809626	16.394560
27.686553	1185.764609	16.399578
27.952153	1159.544441	16.404595
27.485922	1155.026884	16.409613
27.352593	1151.962528	16.414631
27.550149	1166.007568	16.419648
27.769693	1184.211293	16.424666
28.204052	1178.824747	16.429683
27.542102	1168.327923	16.434701
28.049426	1170.717010	16.439719
27.654586	1153.555301	16.444736
27.609342	1171.558322	16.449754
28.163275	1169.829363	16.454771
27.815292	1174.006371	16.459789
27.719432	1164.086167	16.464807
27.636439	1170.552855	16.469824
27.892008	1170.375315	16.474842
28.095331	1166.590670	16.479859
27.886563	1181.666097	16.484877
28.041416	1182.747516	16.489895
28.248294	1186.495882	16.494912
28.229785	1176.430429	16.499930
28.017055	1172.151637	16.504947
28.317354	1185.692986	16.509965
27.820734	1173.474627	16.514983
28.441952	1175.530969	16.520000
28.017005	1180.701441	16.525018
28.274991	1170.642063	16.530035
28.128713	1181.456686	16.535053
28.255003	1168.246367	16.540071
28.203569	1173.302562	16.545088
28.027189	1185.392031	16.550106
28.436221	1173.408199	16.555123
28.309098	1181.830681	16.560141
28.282650	1173.270035	16.565159
28.351281	1183.950932	16.570176
28.403620	1207.514905	16.575194
28.621289	1206.395948	16.580211
28.882137	1194.873918	16.585229
28.636476	1199.503042	16.590247
28.714782	1184.202360	16.595264
28.528002	1190.519896	16.600282
28.741317	1197.114372	16.605299
28.824469	1200.624766	16.610317
28.595133	1200.135887	16.615335
28.968530	1201.480553	16.620352
28.591138	1205.243206	16.625370
28.809964	1200.935603	16.630387
28.800751	1213.145870	16.635405
28.576268	1201.953996	16.640423
28.893435	1196.000291	16.645440
29.060151	1209.728670	16.650458
28.816799	1204.640692	16.655475
28.789941	1194.945050	16.660493
28.587618	1214.287249	16.665511
28.846242	1205.974506	16.670528
28.974858	1209.971993	16.675546
28.980586	1210.867068	16.680563
28.679870	1201.155468	16.685581
28.696333	1223.740515	16.690599
29.366534	1227.653822	16.695616
29.592980	1218.501448	16.700634
29.912011	1214.988370	16.705651
29.807693	1200.977095	16.710669
29.498655	1196.695514	16.715687
29.737636	1196.299886	16.720704
29.600502	1196.126818	16.725722
29.432058	1182.954564	16.730739
29.782112	1189.369380	16.735757
29.313029	1189.005145	16.740775
29.670589	1183.568503	16.745792
29.454834	1199.339673	16.750810
29.531098	1187.611576	16.755827
29.468306	1188.506755	16.760845
29.407808	1189.753465	16.765863
29.575414	1178.053187	16.770880
29.029736	1178.123195	16.775898
29.437917	1186.410179	16.780915
29.783249	1186.902536	16.785933
29.193134	1187.163125	16.790951
29.614784	1195.774607	16.795968
29.827074	1214.767431	16.800986
29.874829	1209.875006	16.806003
29.826520	1216.255877	16.811021
29.897990	1220.084886	16.816039
30.244191	1215.275402	16.821056
30.023307	1217.287082	16.826074
29.963789	1224.383668	16.831091
30.257325	1217.877061	16.836109
29.923152	1225.843705	16.841127
29.970931	1220.277366	16.846144
29.950291	1228.271320	16.851162
29.908874	1227.877940	16.856179
30.126178	1222.369989	16.861197
29.970729	1226.345537	16.866215
30.075173	1232.203417	16.871232
30.177465	1229.680527	16.876250
30.129321	1213.324508	16.881267
30.076820	1225.259110	16.886285
29.996294	1219.532310	16.891303
30.151628	1223.237637	16.896320
30.490506	1236.223335	16.901338
30.247004	1231.837622	16.906355
30.445062	1229.176878	16.911373
30.402353	1247.007155	16.916391
30.791917	1251.771440	16.921408
30.285445	1247.612220	16.926426
30.510208	1251.216725	16.931443
30.648649	1243.998650	16.936461
30.540315	1250.902560	16.941479
31.027028	1244.504744	16.946496
31.009734	1245.993885	16.951514
30.823165	1231.256136	16.956531
30.770548	1216.095346	16.961549
30.565780	1231.642525	16.966567
30.348577	1232.701193	16.971584
30.508199	1239.158324	16.976602
30.594629	1247.432971	16.981619
30.910195	1255.551273	16.986637
30.750922	1249.372589	16.991655
31.163182	1246.382004	16.996672
31.019723	1251.804951	17.001690
30.769578	1256.047689	17.006707
31.018619	1244.397870	17.011725
30.686667	1253.141989	17.016743
30.948365	1249.267768	17.021760
30.670118	1258.452746	17.026778
31.051447	1268.837383	17.031795
31.607550	1269.736968	17.036813
31.410578	1277.138729	17.041831
31.103479	1265.289308	17.046848
31.532320	1268.116313	17.051866
31.168714	1271.235467	17.056883
31.626196	1264.795040	17.061901
31.474370	1271.411902	17.066919
31.385801	1251.717386	17.071936
31.407317	1241.928891	17.076954
31.401878	1263.092846	17.081971
31.694161	1271.884779	17.086989
31.310365	1278.005220	17.092007
31.338436	1271.999276	17.097024
31.890907	1277.606196	17.102042
31.510233	1275.167045	17.107059
31.991884	1276.921911	17.112077
31.961964	1271.069032	17.117095
31.979217	1270.608484	17.122112
31.848120	1267.027873	17.127130
31.785125	1251.643799	17.132147
31.825837	1248.013938	17.137165
31.587317	1259.520128	17.142183
31.683818	1259.551916	17.147200
31.999705	1263.998709	17.152218
31.833106	1269.556370	17.157235
32.245836	1259.159010	17.162253
31.975446	1279.241754	17.167271
32.001977	1272.538930	17.172288
31.961267	1269.797380	17.177306
31.907222	1278.328883	17.182323
32.132427	1271.858147	17.187341
31.817565	1272.089192	17.192359
32.238320	1270.743394	17.197376
32.036995	1270.386870	17.202394
31.699560	1264.949910	17.207411
32.119224	1254.891117	17.212429
31.844124	1273.818714	17.217447
32.354660	1277.418907	17.222464
32.435401	1273.741880	17.227482
32.272298	1284.844940	17.232499
32.261189	1294.027717	17.237517
31.976494	1289.376593	17.242535
32.496146	1280.760675	17.247552
32.286542	1277.000546	17.252570
32.307746	1282.355945	17.257587
32.316216	1275.587414	17.262605
32.127312	1285.116642	17.267623
32.446906	1289.530158	17.272640
32.774452	1308.368837	17.277658
32.902648	1320.662371	17.282675
33.271772	1301.384401	17.287693
32.592976	1303.144649	17.292711
32.722397	1302.418162	17.297728
33.254203	1304.735520	17.302746
32.663950	1306.621271	17.307763
33.271895	1292.931116	17.312781
33.350285	1287.393548	17.317799
33.332578	1279.461416	17.322816
33.248931	1277.505183	17.327834
33.179006	1273.417690	17.332851
33.332734	1262.336866	17.337869
33.091866	1269.263671	17.342887
32.861505	1270.956108	17.347904
33.148070	1271.829774	17.352922
32.949118	1282.867706	17.357939
33.151640	1268.824163	17.362957
33.080128	1273.838441	17.367975
33.041598	1290.758380	17.372992
33.501485	1298.862893	17.378010
33.348970	1304.766807	17.383027
33.332915	1299.912846	17.388045
33.352730	1300.037807	17.393063
33.546087	1304.186405	17.398080
33.447558	1307.235782	17.403098
33.299510	1298.557780	17.408115
33.144971	1302.266703	17.413133
33.005771	1308.250294	17.418151
33.248145	1302.402398	17.423168
33.517545	1305.043784	17.428186
33.498618	1325.752644	17.433203
33.741957	1325.139398	17.438221
33.477348	1331.835347	17.443239
33.243995	1332.319812	17.448256
33.955196	1317.197634	17.453274
33.649900	1327.170662	17.458291
33.871610	1332.697636	17.463309
34.043244	1331.327066	17.468327
33.895707	1329.209365	17.473344
34.185335	1322.415608	17.478362
33.940340	1329.533250	17.483379
34.225308	1318.475376	17.488397
34.135579	1327.010244	17.493415
34.202241	1328.079086	17.498432
34.093185	1314.545188	17.503450
33.813471	1325.306974	17.508467
34.441674	1330.367229	17.513485
34.648602	1329.107935	17.518503
34.233481	1328.138612	17.523520
34.518401	1319.866337	17.528538
34.158337	1328.933402	17.533555
34.294686	1313.086666	17.538573
34.336637	1314.756939	17.543591
34.431803	1348.232388	17.548608
34.634185	1346.364685	17.553626
34.456681	1355.682460	17.558643
34.148517	1345.279584	17.563661
34.431667	1359.144738	17.568679
34.470762	1356.371286	17.573696
34.671647	1349.117256	17.578714
34.705202	1348.517616	17.583731
34.839677	1342.209853	17.588749
34.831678	1339.024961	17.593767
34.677564	1351.497041	17.598784
34.779616	1347.587180	17.603802
34.715990	1351.176973	17.608819
34.607932	1342.508870	17.613837
35.022814	1341.301024	17.618855
34.717425	1360.023135	17.623872
35.014428	1334.879596	17.628890
34.847847	1349.017848	17.633907
35.174294	1368.252784	17.638925
35.350135	1380.125563	17.643943
35.096889	1369.122544	17.648960
35.342079	1365.230750	17.653978
35.078748	1363.766334	17.658995
35.143543	1362.402592	17.664013
35.451771	1373.359334	17.669031
35.612556	1372.003740	17.674048
35.471972	1362.378943	17.679066
35.448099	1368.733402	17.684083
35.503253	1359.170537	17.689101
35.190599	1361.150360	17.694119
35.137361	1370.530666	17.699136
35.518687	1368.974677	17.704154
35.433381	1377.662755	17.709171
35.417729	1370.763938	17.714189
35.754871	1370.924438	17.719207
35.358244	1373.028556	17.724224
35.601596	1370.647071	17.729242
35.609201	1379.224535	17.734259
35.615789	1374.669519	17.739277
35.885990	1373.552695	17.744295
35.350461	1371.452261	17.749312
35.828885	1379.707274	17.754330
35.802941	1393.822719	17.759347
35.699764	1397.374971	17.764365
36.077293	1401.732693	17.769383
36.097368	1404.332632	17.774400
35.930960	1399.547968	17.779418
36.102507	1409.156662	17.784435
35.914339	1404.168734	17.789453
36.628240	1397.891359	17.794471
36.126021	1405.920112	17.799488
36.835078	1394.383896	17.804506
36.490783	1391.832038	17.809523
36.876331	1399.511555	17.814541
36.725069	1384.214560	17.819559
36.428583	1369.029558	17.824576
36.617565	1366.258301	17.829594
36.355685	1365.463030	17.834611
36.476731	1354.942968	17.839629
36.271141	1363.753262	17.844647
36.633044	1375.361074	17.849664
36.816058	1387.373204	17.854682
36.850485	1389.918218	17.859699
36.806038	1381.034691	17.864717
37.008724	1364.836637	17.869735
36.518169	1355.830419	17.874752
36.832037	1361.435270	17.879770
36.899550	1358.983056	17.884787
36.618052	1377.704587	17.889805
37.176173	1371.587197	17.894823
37.055770	1388.479638	17.899840
37.008723	1377.315392	17.904858
36.415008	1366.405444	17.909875
36.729607	1386.372564	17.914893
37.066985	1394.632983	17.919911
36.933494	1392.121672	17.924928
36.925558	1398.729376	17.929946
37.122158	1404.192032	17.934963
36.998238	1387.338190	17.939981
37.307738	1389.356915	17.944999
37.083954	1397.024149	17.950016
36.765400	1388.800389	17.955034
36.801263	1402.566113	17.960051
36.881745	1423.206717	17.965069
37.384657	1421.637125	17.970087
37.027735	1424.657385	17.975104
37.564385	1414.711617	17.980122
37.493068	1422.299345	17.985139
37.320414	1426.656077	17.990157
37.764958	1422.140271	17.995175
37.287556	1421.907503	18.000192
37.755162	1418.014369	18.005210
37.549994	1423.949467	18.010227
37.504583	1443.319953	18.015245
38.137007	1437.699238	18.020263
38.244370	1450.943423	18.025280
38.099619	1441.570409	18.030298
38.091730	1423.226902	18.035315
38.141512	1405.059095	18.040333
38.113785	1412.786443	18.045351
37.912528	1406.415254	18.050368
37.971681	1405.626764	18.055386
38.082350	1416.731915	18.060403
38.032390	1428.003951	18.065421
38.245448	1425.596169	18.070439
38.039907	1444.056446	18.075456
38.172951	1442.791442	18.080474
38.728605	1443.767480	18.085491
38.346444	1441.327564	18.090509
38.639872	1439.311360	18.095527
38.186604	1439.509972	18.100544
38.668970	1449.139956	18.105562
38.439532	1452.293856	18.110579
38.424402	1447.792596	18.115597
38.682486	1442.712804	18.120615
38.579812	1440.394788	18.125632
38.636662	1436.238671	18.130650
38.545431	1443.377011	18.135667
38.525738	1442.280729	18.140685
38.704597	1429.013081	18.145703
38.624864	1446.320849	18.150720
38.808128	1437.863175	18.155738
38.832840	1440.615678	18.160755
38.797576	1439.986862	18.165773
38.867379	1433.748204	18.170791
38.422505	1431.752251	18.175808
38.786440	1444.754651	18.180826
38.840897	1458.737793	18.185843
38.840946	1463.293128	18.190861
39.048120	1454.014093	18.195879
39.178246	1461.317801	18.200896
39.446828	1465.212316	18.205914
39.303631	1475.012414	18.210931
39.219653	1467.174195	18.215949
39.508804	1455.373711	18.220967
39.322923	1477.535944	18.225984
39.354463	1462.607031	18.231002
39.276767	1465.503805	18.236019
39.427186	1472.682923	18.241037
39.533107	1466.422931	18.246055
39.227693	1469.542350	18.251072
39.566505	1464.155158	18.256090
39.635218	1448.245061	18.261107
39.448578	1464.698794	18.266125
39.603344	1461.462180	18.271143
39.445692	1467.646885	18.276160
39.452193	1489.539189	18.281178
40.045100	1487.985030	18.286195
39.653275	1497.470768	18.291213
40.185222	1491.791649	18.296231
39.727168	1490.144863	18.301248
40.070068	1487.017290	18.306266
40.030234	1482.147126	18.311283
40.070756	1489.174555	18.316301
40.611210	1481.453975	18.321319
40.361732	1486.738247	18.326336
40.078340	1481.687693	18.331354
40.287582	1482.832380	18.336371
40.269675	1489.874779	18.341389
40.576243	1485.020194	18.346407
40.416135	1483.919362	18.351424
40.262888	1479.600343	18.356442
40.473918	1480.589048	18.361459
40.288604	1491.683331	18.366477
40.303122	1478.622694	18.371495
40.485910	1484.284679	18.376512
40.139444	1490.113447	18.381530
40.634636	1475.375579	18.386547
40.206433	1484.316613	18.391565
40.161648	1494.922389	18.396583
40.077429	1500.685976	18.401600
40.413056	1508.898722	18.406618
40.403764	1513.732347	18.411635
40.237212	1516.813279	18.416653
40.602730	1528.219851	18.421671
40.646909	1545.336411	18.426688
40.848727	1541.783781	18.431706
41.302886	1537.864497	18.436723
41.353025	1530.640213	18.441741
41.454502	1528.404967	18.446759
41.233649	1538.003794	18.451776
41.554802	1543.268974	18.456794
41.679980	1533.192730	18.461811
41.520271	1523.192502	18.466829
41.408089	1493.334526	18.471847
41.217062	1500.802528	18.476864
41.082716	1498.624953	18.481882
41.526582	1504.881113	18.486899
41.433699	1521.696722	18.491917
41.375715	1528.537129	18.496935
42.033718	1521.503106	18.501952
41.654188	1530.374912	18.506970
42.216298	1520.950385	18.511987
41.770259	1508.425212	18.517005
41.850330	1492.531301	18.522023
41.902073	1491.331098	18.527040
41.481390	1495.093495	18.532058
41.774584	1496.630551	18.537075
41.859312	1511.958347	18.542093
41.909808	1520.620916	18.547111
41.946469	1532.701038	18.552128
41.920496	1527.562071	18.557146
42.283721	1517.250465	18.562163
42.142293	1531.703776	18.567181
41.966596	1522.641098	18.572199
42.153780	1530.896493	18.577216
41.806345	1528.617927	18.582234
42.296517	1526.597345	18.587251
42.091656	1520.097392	18.592269
42.182509	1520.880401	18.597287
42.290016	1523.226183	18.602304
42.095308	1525.584707	18.607322
42.371116	1502.110500	18.612339
42.016095	1526.317393	18.617357
41.775879	1534.471002	18.622375
42.391662	1539.415681	18.627392
42.267065	1551.812780	18.632410
42.542202	1553.598460	18.637427
42.738301	1552.173442	18.642445
42.568421	1556.147129	18.647463
42.647506	1563.757113	18.652480
42.646152	1552.894791	18.657498
42.727993	1565.261723	18.662515
42.853526	1583.675330	18.667533
42.966752	1586.925169	18.672551
43.026677	1588.638361	18.677568
42.933273	1583.595153	18.682586
43.504669	1574.300733	18.687603
43.481267	1576.270377	18.692621
43.477862	1581.595305	18.697639
43.392391	1560.703589	18.702656
43.001201	1544.495429	18.707674
43.327991	1549.998229	18.712691
43.389240	1569.002872	18.717709
43.570662	1574.188805	18.722727
43.658260	1573.685526	18.727744
43.424330	1577.893000	18.732762
43.494953	1581.739167	18.737779
43.622930	1575.557365	18.742797
43.465117	1578.629975	18.747815
43.853397	1576.932482	18.752832
43.695714	1563.220993	18.757850
43.915920	1557.649460	18.762867
43.861806	1573.616120	18.767885
43.556527	1576.200179	18.772903
43.807453	1572.886242	18.777920
43.422218	1576.999247	18.782938
43.672958	1582.101494	18.787955
43.501061	1568.874566	18.792973
43.693789	1573.994860	18.797991
44.086354	1581.913630	18.803008
44.156194	1597.312466	18.808026
44.334948	1599.523275	18.813043
44.173817	1601.083654	18.818061
43.849898	1589.804203	18.823079
44.467920	1602.531515	18.828096
44.150384	1589.395949	18.833114
44.393162	1587.742968	18.838131
44.510770	1599.506069	18.843149
44.661040	1597.187956	18.848167
44.788804	1588.779326	18.853184
44.387666	1599.280304	18.858202
44.544011	1597.806347	18.863219
44.326703	1589.586414	18.868237
44.584056	1596.791023	18.873255
44.576269	1591.848805	18.878272
44.508002	1596.565054	18.883290
44.714997	1608.300597	18.888307
44.810429	1620.490745	18.893325
45.128816	1618.953793	18.898343
45.263497	1612.982650	18.903360
45.058182	1629.333557	18.908378
45.226733	1624.517482	18.913395
45.247969	1611.965198	18.918413
44.980157	1611.045714	18.923431
45.314326	1614.783583	18.928448
45.259086	1618.581670	18.933466
45.232129	1618.282334	18.938483
45.401077	1629.930296	18.943501
45.458262	1630.692500	18.948519
45.639712	1622.441098	18.953536
45.364545	1616.717775	18.958554
45.488987	1620.041152	18.963571
45.273745	1619.215919	18.968589
45.120272	1624.162960	18.973607
45.113115	1626.240737	18.978624
45.459539	1624.170286	18.983642
45.660287	1626.233193	18.988659
45.763897	1636.399246	18.993677
45.495182	1621.218065	18.998695
45.825531	1624.047045	19.003712
45.473302	1632.370771	19.008730
45.307853	1637.122971	19.013747
45.965424	1637.145300	19.018765
45.719688	1650.623770	19.023783
46.009316	1640.350028	19.028800
46.033170	1643.766202	19.033818
46.115120	1645.444073	19.038835
45.912813	1642.243989	19.043853
45.986198	1648.605126	19.048871
46.118876	1662.256672	19.053888
46.165977	1674.150953	19.058906
46.382114	1660.076856	19.063923
46.340807	1670.355056	19.068941
46.292815	1670.986237	19.073959
46.501195	1664.836776	19.078976
46.445385	1669.018776	19.083994
46.583217	1670.397690	19.089011
46.898100	1659.979031	19.094029
46.605885	1680.560916	19.099047
46.675931	1658.487812	19.104064
46.640755	1675.106479	19.109082
46.504361	1674.590809	19.114099
46.907114	1671.547785	19.119117
47.012386	1692.116946	19.124135
47.095499	1693.148258	19.129152
47.422542	1697.641163	19.134170
47.311184	1691.249095	19.139187
47.499890	1690.349036	19.144205
47.167254	1674.243646	19.149223
47.124240	1664.939302	19.154240
46.661897	1669.601419	19.159258
46.998590	1680.206676	19.164275
47.133687	1683.816063	19.169293
47.005650	1688.340275	19.174311
47.277256	1686.077680	19.179328
47.258301	1694.707341	19.184346
47.731090	1706.287042	19.189363
47.946198	1713.551240	19.194381
47.809516	1692.417053	19.199399
48.002806	1683.775524	19.204416
47.853611	1687.978079	19.209434
47.771389	1690.390865	19.214451
48.080762	1674.609050	19.219469
47.471363	1689.158342	19.224487
47.915796	1697.929118	19.229504
48.154079	1709.474356	19.234522
47.820407	1714.555914	19.239539
47.978408	1710.576290	19.244557
47.761787	1724.435003	19.249575
48.090997	1718.948733	19.254592
48.401354	1715.711744	19.259610
47.819852	1716.857609	19.264627
48.093872	1714.288942	19.269645
48.235562	1713.971970	19.274663
48.041042	1719.542673	19.279680
48.157950	1710.839155	19.284698
48.445669	1725.315419	19.289715
48.648240	1734.989458	19.294733
48.521657	1733.800204	19.299751
49.162332	1725.469514	19.304768
48.887419	1726.050609	19.309786
49.072200	1702.869450	19.314803
49.185759	1687.598067	19.319821
48.806534	1697.100936	19.324839
48.795396	1691.812041	19.329856
49.149714	1693.422076	19.334874
48.988641	1696.003188	19.339891
49.163445	1694.797395	19.344909
48.786003	1692.826675	19.349927
49.432718	1689.540604	19.354944
49.170913	1685.252457	19.359962
49.244505	1697.840712	19.364979
49.319361	1692.725180	19.369997
48.952928	1695.604759	19.375015
49.205583	1705.153589	19.380032
49.112691	1731.228064	19.385050
49.352953	1731.325062	19.390067
49.622096	1717.169131	19.395085
49.443905	1725.111830	19.400103
49.451196	1719.333919	19.405120
49.578626	1718.134970	19.410138
49.621129	1724.876389	19.415155
49.720738	1729.146094	19.420173
49.318693	1732.073095	19.425191
49.764118	1732.650887	19.430208
49.669272	1752.754248	19.435226
49.802117	1757.386334	19.440243
50.015093	1754.805900	19.445261
49.543927	1756.397649	19.450279
49.598956	1748.624690	19.455296
49.926140	1756.262069	19.460314
49.862546	1778.137828	19.465331
50.190073	1774.408878	19.470349
50.253604	1784.059474	19.475367
50.742120	1783.309448	19.480384
50.729100	1776.087416	19.485402
50.658117	1780.926793	19.490419
50.692977	1781.864719	19.495437
50.607225	1789.783122	19.500455
50.945938	1782.347077	19.505472
50.881922	1779.341605	19.510490
50.508050	1776.262155	19.515507
51.131204	1772.798291	19.520525
51.071766	1778.966497	19.525543
50.942343	1778.568750	19.530560
51.082076	1776.435597	19.535578
50.959278	1785.138564	19.540595
51.119542	1769.600360	19.545613
51.007932	1776.345421	19.550631
50.943142	1774.993216	19.555648
51.210754	1775.441358	19.560666
51.055885	1774.201861	19.565683
51.107760	1777.909854	19.570701
50.813317	1760.386822	19.575719
51.020146	1781.636477	19.580736
51.017862	1773.617693	19.585754
51.151281	1791.418709	19.590771
51.510911	1793.440424	19.595789
51.760440	1813.155501	19.600807
51.826505	1808.600172	19.605824
51.645162	1809.194544	19.610842
51.685072	1810.294807	19.615859
52.279116	1798.309640	19.620877
51.828223	1798.202584	19.625895
51.645423	1798.931038	19.630912
52.417115	1789.883082	19.635930
51.832419	1796.008779	19.640947
52.150347	1797.101085	19.645965
52.003435	1795.447330	19.650983
51.991955	1793.068724	19.656000
52.186140	1788.022800	19.661018
51.999292	1800.305205	19.666035
52.293475	1791.599508	19.671053
51.923711	1789.308452	19.676071
52.175560	1796.896497	19.681088
52.276450	1797.793005	19.686106
52.046013	1792.064587	19.691123
52.157624	1801.119723	19.696141
52.033333	1824.525270	19.701159
52.343333	1809.240595	19.706176
52.723691	1821.808570	19.711194
52.327598	1826.233829	19.716211
52.652728	1822.794993	19.721229
52.624870	1828.005951	19.726247
52.714657	1854.338600	19.731264
53.364646	1842.127448	19.736282
53.194438	1850.089755	19.741299
53.372474	1845.748365	19.746317
53.323518	1836.033138	19.751335
53.128505	1832.454690	19.756352
53.551400	1825.235198	19.761370
53.365252	1821.302771	19.766387
53.627390	1806.606054	19.771405
53.231744	1806.522936	19.776423
53.339967	1815.130664	19.781440
53.421449	1820.073583	19.786458
53.393618	1830.346907	19.791475
53.429090	1820.627776	19.796493
53.830419	1840.822466	19.801511
53.666507	1837.809280	19.806528
53.880620	1834.312221	19.811546
53.634874	1841.090105	19.816563
53.690355	1829.764315	19.821581
53.938979	1838.733454	19.826599
53.593965	1834.505268	19.831616
53.944849	1836.867960	19.836634
53.728750	1840.355126	19.841651
53.943464	1858.594699	19.846669
54.100771	1864.288789	19.851687
54.071837	1874.479264	19.856704
54.402869	1862.102917	19.861722
54.265623	1864.302999	19.866739
54.030178	1870.147416	19.871757
54.379493	1868.348274	19.876775
54.095082	1869.112614	19.881792
54.213491	1875.526240	19.886810
54.632732	1880.546025	19.891827
55.207892	1887.298301	19.896845
54.747403	1883.856022	19.901863
54.758983	1882.425250	19.906880
54.946571	1878.606422	19.911898
54.664432	1891.874412	19.916915
55.181886	1888.289227	19.921933
55.019656	1875.867427	19.926951
55.018249	1887.095953	19.931968
55.339447	1873.672134	19.936986
55.205434	1879.268325	19.942003
55.536555	1881.593153	19.947021
55.647626	1887.962136	19.952039
55.379989	1873.195832	19.957056
55.089970	1868.258240	19.962074
55.127351	1881.486214	19.967091
55.241840	1873.583696	19.972109
55.300464	1885.727781	19.977127
55.371918	1886.089263	19.982144
55.238289	1864.146754	19.987162
55.379794	1884.373414	19.992179
55.427362	1893.332114	19.997197
55.588247	1899.508246	20.002215
55.673667	1897.848170	20.007232
56.288528	1910.647513	20.012250
56.060195	1908.262406	20.017267
56.054099	1902.989336	20.022285
56.279252	1897.922513	20.027303
56.150085	1910.368090	20.032320
56.143480	1893.586029	20.037338
55.969392	1913.484412	20.042355
56.431400	1914.003180	20.047373
56.616369	1900.756161	20.052391
56.105951	1908.678863	20.057408
56.628930	1902.152162	20.062426
56.440564	1902.850442	20.067443
56.430769	1900.950028	20.072461
56.455305	1902.059529	20.077479
56.118284	1919.846515	20.082496
56.312874	1924.558990	20.087514
56.203825	1940.816769	20.092531
56.689908	1935.484400	20.097549
56.714121	1932.617449	20.102567
56.372659	1937.513184	20.107584
57.100230	1947.179333	20.112602
57.050594	1963.214940	20.117619
57.138102	1957.277244	20.122637
57.484362	1950.705915	20.127655
57.298670	1957.561121	20.132672
57.665837	1950.736366	20.137690
57.553617	1955.049405	20.142707
57.616290	1947.183755	20.147725
57.847440	1946.429800	20.152743
57.703339	1956.301014	20.157760
57.771253	1957.081735	20.162778
57.838712	1944.836268	20.167795
57.781035	1952.798928	20.172813
58.025031	1935.133577	20.177831
57.982142	1943.180786	20.182848
57.866837	1939.407863	20.187866
57.746957	1941.131124	20.192883
57.644184	1948.515868	20.197901
58.056636	1939.112867	20.202919
57.541021	1937.835736	20.207936
57.793078	1945.281121	20.212954
57.959847	1955.305467	20.217971
58.456061	1962.702247	20.222989
58.462269	1976.428902	20.228007
58.375873	1987.391854	20.233024
58.298481	1977.215738	20.238042
58.387424	1973.250805	20.243059
58.418322	1975.726035	20.248077
58.654216	1967.308187	20.253095
58.397947	1976.143344	20.258112
58.735185	1969.848664	20.263130
58.835167	1968.777249	20.268147
58.645901	1975.142164	20.273165
58.694236	1979.113360	20.278183
58.788073	1991.659144	20.283200
58.420910	1996.250714	20.288218
58.999778	1995.651085	20.293235
58.853702	1989.533497	20.298253
59.017746	1990.448908	20.303271
58.846704	2001.581941	20.308288
59.336971	1997.257803	20.313306
59.489536	2022.107892	20.318323
59.156451	2033.762357	20.323341
59.358827	2028.279813	20.328359
59.402284	2028.156214	20.333376
59.399783	2030.674960	20.338394
59.439571	2029.410557	20.343411
59.350525	2033.701483	20.348429
59.499837	2025.198907	20.353447
59.599718	2052.034895	20.358464
60.046075	2057.940122	20.363482
60.259099	2059.133830	20.368499
60.116121	2058.049216	20.373517
60.229249	2050.139747	20.378535
60.337697	2053.150737	20.383552
60.921895	2048.153260	20.388570
60.378653	2030.184866	20.393587
60.332356	2026.965810	20.398605
60.360329	2027.015027	20.403623
60.218403	2033.269005	20.408640
60.555350	2047.676619	20.413658
60.709695	2051.487811	20.418675
60.396407	2047.818829	20.423693
60.584349	2046.821840	20.428711
60.562432	2045.580426	20.433728
60.620312	2048.807427	20.438746
60.965508	2039.233215	20.443763
60.764463	2052.118101	20.448781
61.060437	2038.648116	20.453799
60.805597	2053.924900	20.458816
60.834983	2063.160099	20.463834
61.023163	2068.502153	20.468851
60.963334	2077.809971	20.473869
61.051978	2080.999024	20.478887
61.024068	2085.010796	20.483904
61.137350	2074.476764	20.488922
61.339369	2092.986007	20.493939
61.231062	2100.777010	20.498957
61.564456	2096.009329	20.503975
61.505201	2102.851776	20.508992
61.960971	2099.765267	20.514010
61.942433	2095.159865	20.519027
61.921379	2096.280654	20.524045
62.234666	2095.022030	20.529063
61.988377	2095.906446	20.534080
61.821991	2094.875102	20.539098
62.580371	2090.116517	20.544115
61.980693	2102.141233	20.549133
62.239071	2096.509859	20.554151
62.004220	2092.823181	20.559168
61.956326	2097.445675	20.564186
62.305711	2115.822731	20.569203
62.239375	2129.405620	20.574221
62.355878	2124.520834	20.579239
62.705434	2126.371246	20.584256
62.542767	2128.636386	20.589274
62.731011	2118.412738	20.594291
62.739027	2132.113449	20.599309
63.116074	2118.790020	20.604327
62.594054	2119.059833	20.609344
63.054707	2122.775943	20.614362
63.422075	2108.327467	20.619379
63.238873	2117.619873	20.624397
62.986690	2125.836197	20.629415
63.044591	2128.713051	20.634432
63.233641	2131.943784	20.639450
63.529963	2144.111189	20.644467
63.028549	2150.164015	20.649485
63.489372	2150.115133	20.654503
63.425895	2154.900045	20.659520
63.424885	2148.619460	20.664538
63.608877	2142.764951	20.669555
63.346669	2151.496476	20.674573
63.329931	2143.684593	20.679591
63.863750	2148.041504	20.684608
63.518506	2158.805446	20.689626
64.125004	2162.307327	20.694643
64.068030	2180.845695	20.699661
64.395655	2173.660288	20.704679
64.370749	2179.819601	20.709696
64.453583	2175.704853	20.714714
64.613385	2186.406615	20.719731
64.198594	2166.162729	20.724749
64.193831	2164.771242	20.729767
64.065060	2176.928021	20.734784
64.097779	2179.678349	20.739802
64.250197	2167.910350	20.744819
63.947571	2182.529477	20.749837
64.173255	2187.359520	20.754855
64.494134	2182.421260	20.759872
64.670072	2198.821371	20.764890
64.690814	2198.343883	20.769907
64.446647	2216.423118	20.774925
64.743426	2226.306877	20.779943
65.417560	2225.594460	20.784960
65.346625	2232.746148	20.789978
65.427383	2226.193382	20.794995
65.398124	2230.653403	20.800013
65.850310	2218.179397	20.805031
65.837778	2221.540892	20.810048
65.665100	2219.828756	20.815066
65.774165	2212.976859	20.820083
65.257533	2222.936178	20.825101
65.636378	2216.627436	20.830119
65.559396	2224.167287	20.835136
65.912287	2225.600468	20.840154
65.892732	2214.398988	20.845171
65.448123	2216.680223	20.850189
65.674904	2228.305106	20.855207
65.783262	2240.549116	20.860224
65.813823	2256.618032	20.865242
65.805132	2256.073758	20.870259
65.821586	2257.307641	20.875277
66.069837	2274.685160	20.880295
66.717793	2274.085128	20.885312
66.397654	2276.152316	20.890330
66.756525	2272.357052	20.895347
66.804860	2277.605173	20.900365
66.882589	2276.761409	20.905383
66.762642	2275.704467	20.910400
66.944227	2280.204063	20.915418
67.149514	2262.188469	20.920435
66.925566	2277.862497	20.925453
67.095816	2274.013173	20.930471
67.125743	2270.306318	20.935488
67.098235	2256.480778	20.940506
67.386479	2264.788367	20.945523
67.047578	2275.500953	20.950541
67.115378	2265.933665	20.955559
67.425488	2266.153760	20.960576
67.525739	2269.308260	20.965594
67.455050	2263.006074	20.970611
67.416759	2275.567231	20.975629
67.296159	2283.634545	20.980647
67.760155	2297.937549	20.985664
67.512234	2306.545354	20.990682
67.873666	2289.301098	20.995699
67.959134	2295.872493	21.000717
68.067578	2304.959155	21.005735
68.049628	2288.772775	21.010752
67.770398	2287.873441	21.015770
68.432109	2280.159593	21.020787
68.182341	2288.694078	21.025805
68.208821	2291.645833	21.030823
68.499876	2300.163193	21.035840
68.517875	2325.058052	21.040858
68.590524	2317.554902	21.045875
68.829749	2317.349939	21.050893
68.797729	2327.587085	21.055911
68.855855	2316.886034	21.060928
68.925802	2314.595261	21.065946
68.972463	2311.374562	21.070963
68.996659	2321.456759	21.075981
69.287872	2321.282179	21.080999
69.335436	2320.045598	21.086016
68.691558	2310.951365	21.091034
69.000081	2316.132885	21.096051
69.063867	2312.329685	21.101069
69.157094	2318.471894	21.106087
69.164738	2324.760323	21.111104
69.414389	2337.631594	21.116122
69.120247	2338.265292	21.121139
69.419874	2345.919921	21.126157
69.434045	2336.417746	21.131175
69.746172	2339.969887	21.136192
69.614717	2353.475160	21.141210
70.363206	2347.645787	21.146227
70.413711	2361.572336	21.151245
70.504629	2366.907144	21.156263
70.539686	2335.649307	21.161280
70.121784	2340.672750	21.166298
70.217622	2333.608634	21.171315
70.251548	2343.622511	21.176333
70.704711	2363.823298	21.181351
70.681105	2369.288636	21.186368
70.762624	2372.911960	21.191386
70.495446	2358.530317	21.196403
70.706592	2367.216417	21.201421
70.644763	2365.990627	21.206439
70.731744	2351.289465	21.211456
70.658548	2361.703108	21.216474
70.366760	2364.988547	21.221491
70.661898	2367.166655	21.226509
70.678177	2384.299387	21.231527
71.109077	2380.968531	21.236544
70.978581	2384.883957	21.241562
71.165793	2382.937740	21.246579
71.265281	2388.049308	21.251597
71.134909	2404.219570	21.256615
71.814858	2415.790575	21.261632
71.816765	2428.699122	21.266650
71.448550	2421.763022	21.271667
71.778922	2416.497950	21.276685
71.708100	2414.860685	21.281703
71.688635	2412.135695	21.286720
71.750195	2417.608628	21.291738
71.565044	2408.147613	21.296755
71.877428	2424.714181	21.301773
71.897645	2441.145007	21.306791
71.890647	2435.322736	21.311808
71.925427	2446.117773	21.316826
72.081795	2439.860468	21.321843
72.484447	2456.843614	21.326861
72.835343	2474.082359	21.331879
73.089096	2449.961197	21.336896
72.964786	2438.919964	21.341914
72.789614	2443.527376	21.346931
72.644162	2447.131929	21.351949
72.682164	2447.143469	21.356967
73.273620	2456.099424	21.361984
73.136528	2472.878103	21.367002
73.072284	2459.039950	21.372019
73.386263	2464.421389	21.377037
73.291570	2460.666189	21.382055
73.614693	2451.236502	21.387072
73.523840	2462.880196	21.392090
73.374254	2465.888635	21.397107
73.538500	2461.256068	21.402125
73.561114	2472.299964	21.407143
73.569725	2463.245641	21.412160
73.245960	2461.854286	21.417178
73.433684	2462.644956	21.422195
73.564677	2478.886665	21.427213
73.604505	2485.064731	21.432231
74.022383	2488.554160	21.437248
73.870997	2490.460627	21.442266
73.961880	2486.120075	21.447283
74.105313	2492.126903	21.452301
74.014383	2515.211277	21.457319
73.786458	2514.883326	21.462336
73.929860	2524.127320	21.467354
74.697036	2512.505682	21.472371
74.544929	2528.583610	21.477389
74.725200	2544.657217	21.482407
75.243113	2539.351862	21.487424
75.164529	2542.612736	21.492442
75.219677	2548.390689	21.497459
75.150438	2530.634304	21.502477
75.136222	2543.245830	21.507495
75.400908	2542.601849	21.512512
75.400976	2537.560006	21.517530
75.413909	2531.687165	21.522547
75.678644	2529.536403	21.527565
75.731918	2539.749163	21.532583
75.725615	2537.658737	21.537600
75.706260	2535.883043	21.542618
75.492058	2533.901770	21.547635
75.684033	2533.998488	21.552653
75.828640	2528.179475	21.557671
75.808930	2538.745607	21.562688
76.107329	2534.879963	21.567706
75.716657	2535.634139	21.572723
76.016713	2557.970950	21.577741
75.760650	2568.210241	21.582759
76.463129	2561.785288	21.587776
76.421025	2570.708612	21.592794
76.321681	2576.071980	21.597811
76.524417	2562.258903	21.602829
76.374137	2567.749967	21.607847
76.616595	2587.708526	21.612864
76.782466	2583.808671	21.617882
76.904308	2587.119500	21.622899
77.035153	2597.527535	21.627917
76.920973	2590.115555	21.632935
77.107435	2574.797983	21.637952
77.215897	2589.767839	21.642970
77.148562	2597.040351	21.647987
77.449930	2590.115568	21.653005
77.319118	2593.865363	21.658023
77.237104	2590.358412	21.663040
77.480527	2590.033273	21.668058
76.713258	2600.990676	21.673075
77.338383	2611.436522	21.678093
77.390130	2619.656227	21.683111
77.533790	2617.187098	21.688128
78.081637	2610.568205	21.693146
77.417443	2613.223355	21.698163
77.464017	2635.343718	21.703181
77.990374	2637.196866	21.708199
78.092487	2639.294516	21.713216
78.260060	2639.677137	21.718234
78.387047	2637.108406	21.723251
78.425424	2636.235695	21.728269
78.601717	2639.678078	21.733287
78.691484	2650.114589	21.738304
78.906685	2642.941047	21.743322
79.206392	2664.539342	21.748339
79.092350	2654.363718	21.753357
78.997441	2643.274569	21.758375
79.140513	2650.154291	21.763392
79.410244	2649.852362	21.768410
79.293402	2645.674429	21.773427
79.548377	2628.327907	21.778445
79.535429	2638.380034	21.783463
79.093748	2632.341350	21.788480
79.342301	2656.630575	21.793498
79.397470	2665.568980	21.798515
79.834139	2653.849107	21.803533
79.387151	2668.292954	21.808551
79.312293	2668.458765	21.813568
79.476524	2674.226612	21.818586
79.835321	2691.321785	21.823603
80.158310	2687.058563	21.828621
80.045303	2695.253765	21.833639
80.020442	2688.740105	21.838656
80.110800	2678.499589	21.843674
80.084019	2684.785192	21.848691
80.115045	2692.497370	21.853709
80.091227	2716.147293	21.858727
80.386942	2706.788709	21.863744
80.802573	2715.303233	21.868762
80.604556	2714.951832	21.873779
80.827304	2722.350079	21.878797
80.968433	2708.086846	21.883815
81.122342	2712.588191	21.888832
81.468724	2713.404623	21.893850
80.802638	2714.597008	21.898867
80.877761	2719.625907	21.903885
81.232250	2733.841317	21.908903
81.603321	2728.037953	21.913920
82.171788	2736.139660	21.918938
81.568756	2733.997430	21.923955
81.755244	2748.001260	21.928973
81.393742	2737.401147	21.933991
81.606631	2740.277699	21.939008
82.100354	2740.707210	21.944026
81.926291	2728.945100	21.949043
81.966279	2733.766633	21.954061
82.413858	2758.490030	21.959079
82.292691	2763.412608	21.964096
82.608403	2756.464123	21.969114
82.284022	2765.232248	21.974131
82.767056	2752.187595	21.979149
82.627101	2757.022730	21.984167
82.565754	2763.993956	21.989184
82.676681	2757.527313	21.994202
82.438016	2761.330401	21.999219
82.864359	2759.365685	22.004237
82.831994	2756.722091	22.009255
82.812042	2759.519807	22.014272
82.628312	2758.413729	22.019290
82.589870	2782.366742	22.024307
83.105824	2774.162793	22.029325
83.049708	2776.877517	22.034343
83.226387	2786.602950	22.039360
83.476237	2777.349731	22.044378
83.216046	2801.802381	22.049395
83.652606	2808.928345	22.054413
83.641084	2801.344584	22.059431
83.537412	2814.855116	22.064448
83.744060	2808.845835	22.069466
83.445506	2822.985786	22.074483
83.894423	2833.084349	22.079501
83.501967	2843.055037	22.084519
83.818373	2843.672898	22.089536
84.360892	2832.235973	22.094554
84.185100	2841.913392	22.099571
84.718678	2859.338905	22.104589
84.961869	2853.479859	22.109607
85.042268	2863.437774	22.114624
85.263041	2863.308489	22.119642
85.049892	2853.332565	22.124659
85.232103	2842.713790	22.129677
85.178532	2837.902550	22.134695
85.274468	2842.027510	22.139712
85.739612	2838.714717	22.144730
85.125493	2842.663326	22.149747
85.339333	2839.160183	22.154765
85.440550	2847.886766	22.159783
85.510333	2852.553028	22.164800
85.600959	2847.814802	22.169818
85.256055	2854.966383	22.174835
85.494817	2846.884180	22.179853
85.514673	2861.950630	22.184871
85.565099	2892.276962	22.189888
85.881229	2868.271804	22.194906
85.618142	2883.228738	22.199923
85.634923	2883.332757	22.204941
86.050805	2902.015495	22.209959
85.867035	2914.047696	22.214976
86.559040	2911.431220	22.219994
86.684501	2911.183046	22.225011
86.527801	2908.042676	22.230029
86.749025	2916.486489	22.235047
87.021467	2938.418002	22.240064
87.352195	2941.434166	22.245082
87.093058	2947.052795	22.250099
87.218794	2932.829300	22.255117
87.377575	2935.219973	22.260135
87.387905	2938.717799	22.265152
87.472983	2927.868572	22.270170
87.164379	2934.892150	22.275187
87.239524	2936.541170	22.280205
87.542034	2943.227953	22.285223
86.954265	2934.203993	22.290240
87.696176	2950.740503	22.295258
87.372731	2966.210615	22.300275
88.010112	2956.871206	22.305293
87.900465	2959.648742	22.310311
87.976052	2967.648167	22.315328
88.430681	2965.601590	22.320346
88.355931	2984.421011	22.325363
88.219727	2993.137698	22.330381
88.607579	2979.001943	22.335399
88.208981	2992.518846	22.340416
88.583964	2992.617216	22.345434
88.655511	2975.789374	22.350451
88.637648	2987.384787	22.355469
89.014459	2989.500870	22.360487
88.533915	2992.852274	22.365504
89.342430	3007.074010	22.370522
89.264266	3004.584391	22.375539
89.275586	3002.115812	22.380557
89.589642	3011.415162	22.385575
89.429416	3002.126034	22.390592
89.865576	3005.892863	22.395610
89.934644	3006.062649	22.400627
89.829665	3005.594691	22.405645
89.968649	3000.016970	22.410663
89.904446	3006.525020	22.415680
89.777354	2996.807210	22.420698
89.995618	3013.091356	22.425715
89.685828	3001.325877	22.430733
90.086761	3010.130972	22.435751
90.035812	3034.206514	22.440768
90.105095	3029.105634	22.445786
90.247147	3033.236804	22.450803
90.062851	3034.731865	22.455821
90.632941	3052.382655	22.460839
90.492285	3066.884908	22.465856
90.882768	3073.817436	22.470874
90.803159	3063.944107	22.475891
90.979293	3059.192081	22.480909
91.357457	3065.169596	22.485927
91.020332	3064.984080	22.490944
91.453565	3065.056685	22.495962
91.856188	3085.504753	22.500979
91.988993	3082.113367	22.505997
92.001480	3080.587850	22.511015
91.978422	3074.209748	22.516032
91.832713	3066.213403	22.521050
91.884036	3070.616258	22.526067
91.633524	3083.575722	22.531085
92.045603	3072.467643	22.536103
92.178645	3082.756751	22.541120
92.098904	3074.677456	22.546138
91.979578	3081.587543	22.551155
92.113847	3105.331421	22.556173
91.940175	3110.828117	22.561191
92.297155	3113.647859	22.566208
92.776899	3111.215239	22.571226
92.754635	3107.622316	22.576243
92.403913	3125.322202	22.581261
92.875418	3129.311560	22.586279
93.075931	3135.645611	22.591296
93.144420	3135.258428	22.596314
93.075606	3135.989168	22.601331
92.977895	3153.700819	22.606349
93.219930	3153.918007	22.611367
93.502998	3173.007257	22.616384
93.623699	3162.431104	22.621402
94.201666	3172.314085	22.626419
93.688408	3170.329391	22.631437
94.278507	3156.565553	22.636455
94.222029	3169.075324	22.641472
93.899375	3164.824176	22.646490
94.295621	3158.888939	22.651507
94.283445	3167.451375	22.656525
94.356721	3175.445778	22.661543
94.241989	3188.156129	22.666560
94.535782	3183.181874	22.671578
94.691877	3184.069539	22.676595
94.587164	3186.225456	22.681613
94.890345	3185.054635	22.686631
94.618738	3189.607732	22.691648
95.257852	3178.958502	22.696666
94.980195	3196.186175	22.701683
95.036032	3208.429396	22.706701
95.596407	3211.470657	22.711719
95.488978	3222.846409	22.716736
95.442217	3208.348419	22.721754
95.451863	3218.146999	22.726771
95.472614	3211.919077	22.731789
95.252901	3205.805693	22.736807
95.757555	3226.427239	22.741824
95.748681	3230.944414	22.746842
95.738114	3237.387793	22.751859
95.845450	3262.697731	22.756877
96.045072	3243.425673	22.761895
96.122278	3259.027896	22.766912
96.227447	3286.665327	22.771930
96.304440	3276.106949	22.776947
96.281057	3275.803840	22.781965
96.911530	3272.834493	22.786983
96.642064	3276.849482	22.792000
96.940806	3284.963768	22.797018
97.212079	3303.108698	22.802035
97.006214	3299.621263	22.807053
97.612206	3289.715600	22.812071
97.310236	3299.901935	22.817088
97.501583	3290.137621	22.822106
97.553028	3293.561806	22.827123
97.792173	3302.314671	22.832141
97.487902	3284.238001	22.837159
97.848466	3308.607771	22.842176
97.787203	3319.113783	22.847194
98.038709	3322.381298	22.852211
97.882378	3328.396450	22.857229
97.872280	3330.140305	22.862247
97.859950	3334.787999	22.867264
98.020100	3357.457148	22.872282
98.454284	3352.605307	22.877299
98.620667	3354.823140	22.882317
98.735652	3348.444555	22.887335
98.682934	3361.318024	22.892352
98.605214	3361.340814	22.897370
99.122312	3377.482659	22.902387
98.898104	3377.693824	22.907405
98.844973	3387.841855	22.912423
99.163916	3388.647506	22.917440
99.136234	3387.360087	22.922458
99.851598	3387.405366	22.927475
99.328679	3407.689483	22.932493
100.035895	3404.765697	22.937511
99.490994	3418.150849	22.942528
99.618445	3417.455104	22.947546
100.135513	3399.665799	22.952563
99.985940	3414.584408	22.957581
100.230172	3410.689115	22.962599
100.580173	3411.187673	22.967616
100.233623	3433.550118	22.972634
100.853321	3435.282434	22.977651
100.578512	3439.724324	22.982669
100.668523	3439.599321	22.987687
100.827070	3446.672705	22.992704
100.679629	3448.947133	22.997722
100.730024	3446.463758	23.002739
100.821314	3457.642675	23.007757
101.069544	3464.444558	23.012775
101.454836	3462.048359	23.017792
101.497180	3465.861875	23.022810
101.723733	3462.272635	23.027827
101.514021	3476.572118	23.032845
101.723227	3457.625371	23.037863
101.762911	3466.745535	23.042880
101.602720	3466.159128	23.047898
101.545978	3469.014625	23.052915
101.867221	3480.702402	23.057933
101.903540	3488.697955	23.062951
102.064947	3482.187238	23.067968
101.752155	3493.282954	23.072986
102.448467	3500.034039	23.078003
102.337177	3519.646749	23.083021
102.759575	3515.598763	23.088039
103.218210	3514.723094	23.093056
102.798666	3516.050382	23.098074
103.101651	3505.625761	23.103091
102.895618	3519.773497	23.108109
102.997460	3513.210799	23.113127
103.107829	3530.103861	23.118144
103.364856	3548.951031	23.123162
103.616143	3539.319962	23.128179
103.241980	3542.883820	23.133197
103.368850	3543.552717	23.138215
103.440460	3555.034559	23.143232
103.722396	3574.113074	23.148250
103.934057	3572.192002	23.153267
104.058953	3567.076638	23.158285
104.210008	3566.520686	23.163303
104.236793	3575.081633	23.168320
104.489962	3592.276754	23.173338
104.636943	3599.968648	23.178355
104.646828	3599.036025	23.183373
104.404242	3593.896337	23.188391
104.689070	3586.895895	23.193408
104.725415	3598.683593	23.198426
104.926727	3611.008604	23.203443
104.993039	3618.074866	23.208461
105.012649	3615.649700	23.213479
104.941726	3623.716981	23.218496
104.701069	3633.361910	23.223514
105.433835	3639.783414	23.228531
105.236313	3655.230646	23.233549
105.609223	3668.099786	23.238567
106.019452	3666.228568	23.243584
106.018796	3674.885443	23.248602
106.208143	3662.742494	23.253619
106.130112	3671.846797	23.258637
106.212793	3680.915887	23.263655
106.760064	3674.831878	23.268672
106.690428	3694.987137	23.273690
106.783478	3692.336045	23.278707
106.641022	3695.345116	23.283725
106.906765	3703.228461	23.288743
107.314721	3687.893469	23.293760
107.185291	3696.533840	23.298778
106.964260	3697.977552	23.303795
107.170996	3692.356893	23.308813
107.470793	3699.220044	23.313831
107.625876	3712.189781	23.318848
107.437093	3720.774225	23.323866
107.735085	3727.182962	23.328883
107.454725	3730.605772	23.333901
107.553385	3727.591936	23.338919
107.766420	3740.029286	23.343936
107.938452	3751.252159	23.348954
108.026776	3757.357365	23.353971
108.252620	3763.472134	23.358989
108.252274	3759.374255	23.364007
108.664655	3774.515706	23.369024
108.681784	3794.039431	23.374042
108.739797	3777.783825	23.379059
108.633332	3787.686204	23.384077
108.900009	3786.818618	23.389095
109.092906	3778.873827	23.394112
108.873020	3786.556357	23.399130
109.150190	3802.977664	23.404147
109.219611	3812.358079	23.409165
109.308633	3821.395889	23.414183
109.589128	3814.432281	23.419200
109.338277	3820.844740	23.424218
109.888040	3834.295035	23.429235
110.391558	3848.092355	23.434253
109.903616	3845.487241	23.439271
110.371689	3841.508397	23.444288
110.124586	3851.495866	23.449306
110.298347	3839.840005	23.454323
110.577322	3839.649916	23.459341
110.337689	3849.965287	23.464359
110.663694	3868.504201	23.469376
110.575073	3870.992988	23.474394
110.816146	3869.195762	23.479411
111.141565	3861.181393	23.484429
111.139249	3879.534413	23.489447
111.550952	3888.213427	23.494464
111.538170	3893.225933	23.499482
111.769499	3901.247744	23.504499
112.087877	3900.554288	23.509517
111.820572	3894.556764	23.514535
111.961416	3899.111599	23.519552
111.892102	3903.618483	23.524570
111.939803	3896.128339	23.529587
112.156962	3903.443824	23.534605
112.153951	3921.731653	23.539623
112.606197	3916.533343	23.544640
112.267323	3923.401340	23.549658
112.618521	3926.112739	23.554675
112.804325	3927.325859	23.559693
112.569841	3930.473018	23.564711
112.759093	3941.301840	23.569728
112.764165	3961.065171	23.574746
112.795643	3955.179673	23.579763
113.058005	3958.784904	23.584781
113.285379	3984.929347	23.589799
113.553090	3973.571645	23.594816
113.609070	3987.522571	23.599834
113.408153	3979.539207	23.604851
113.893093	3991.504657	23.609869
114.070238	4006.319058	23.614887
114.358064	4012.033518	23.619904
114.078332	4010.499108	23.624922
114.184436	4004.030777	23.629939
114.298156	4024.315222	23.634957
114.387989	4035.639680	23.639975
114.954794	4034.143343	23.644992
114.834753	4048.813974	23.650010
114.828532	4043.246882	23.655027
115.378606	4038.860337	23.660045
114.875327	4047.665041	23.665063
115.455063	4046.683899	23.670080
115.360973	4067.826378	23.675098
115.496276	4068.814778	23.680115
115.542373	4059.287768	23.685133
115.539483	4065.425884	23.690151
115.705283	4054.032995	23.695168
116.206094	4066.533293	23.700186
116.045624	4069.382024	23.705203
116.391461	4083.896570	23.710221
116.057946	4093.003570	23.715239
116.395372	4090.266754	23.720256
116.103648	4103.387028	23.725274
116.333735	4099.100586	23.730291
116.563501	4100.247399	23.735309
116.579048	4127.435375	23.740327
116.788342	4119.232972	23.745344
116.983611	4125.897831	23.750362
117.065781	4126.656426	23.755379
117.322591	4130.865386	23.760397
117.173380	4158.138516	23.765415
117.315208	4151.157120	23.770432
117.514286	4157.796561	23.775450
117.424602	4153.911771	23.780467
117.827835	4166.195590	23.785485
117.775979	4179.989305	23.790503
117.878034	4165.935923	23.795520
118.071192	4183.619975	23.800538
117.944465	4193.897624	23.805555
118.797922	4200.398244	23.810573
118.697821	4204.798489	23.815591
118.797313	4204.681363	23.820608
118.731503	4200.365832	23.825626
119.229098	4205.306310	23.830643
119.296803	4195.113815	23.835661
119.254694	4193.819657	23.840679
119.668938	4205.063074	23.845696
119.945594	4224.844465	23.850714
119.901014	4225.537785	23.855731
120.014787	4217.028663	23.860749
119.714520	4219.308769	23.865767
119.919736	4209.471901	23.870784
120.133496	4219.240929	23.875802
120.145892	4225.036021	23.880819
120.339282	4223.384827	23.885837
120.399961	4234.847717	23.890855
120.247317	4254.393773	23.895872
120.575572	4259.341383	23.900890
120.024326	4273.304710	23.905907
120.541208	4266.900287	23.910925
120.346547	4280.859032	23.915943
120.602777	4304.304660	23.920960
120.695943	4311.062851	23.925978
120.812686	4314.967829	23.930995
121.249735	4320.066779	23.936013
121.472120	4335.278364	23.941031
121.935274	4332.738456	23.946048
122.220785	4345.172977	23.951066
121.837491	4347.668797	23.956083
122.325423	4338.065065	23.961101
122.238257	4347.276788	23.966119
122.298766	4357.242886	23.971136
122.681615	4376.334848	23.976154
122.306774	4376.074043	23.981171
122.983420	4375.576497	23.986189
122.746396	4380.157690	23.991207
123.030945	4380.328896	23.996224
122.726797	4384.810153	24.001242
122.788798	4403.047645	24.006259
123.336752	4397.766038	24.011277
123.176117	4396.863512	24.016295
123.560604	4427.519154	24.021312
123.690000	4437.785352	24.026330
123.693802	4437.454892	24.031347
123.730766	4429.323324	24.036365
123.704598	4452.063441	24.041383
123.721123	4466.920569	24.046400
124.275553	4463.159990	24.051418
123.979189	4468.131740	24.056435
124.264359	4478.854532	24.061453
124.820218	4491.281507	24.066471
124.699845	4499.105037	24.071488
125.215281	4495.710754	24.076506
124.547602	4494.745935	24.081523
125.155961	4494.167145	24.086541
124.906605	4497.961395	24.091559
125.332127	4511.126888	24.096576
125.323937	4518.435409	24.101594
125.141057	4520.118966	24.106611
125.705574	4528.049037	24.111629
125.933665	4546.912830	24.116647
125.936074	4551.564358	24.121664
126.092465	4550.134216	24.126682
126.240029	4558.089102	24.131699
126.286262	4565.274472	24.136717
126.143615	4569.346398	24.141735
126.058223	4587.036382	24.146752
126.480454	4591.948097	24.151770
126.546387	4603.272586	24.156787
126.988688	4610.170867	24.161805
127.027078	4620.143937	24.166823
127.292935	4620.243428	24.171840
127.505603	4628.809675	24.176858
127.345584	4652.818337	24.181875
127.633511	4643.734111	24.186893
127.781420	4640.158386	24.191911
127.800389	4647.644774	24.196928
128.329944	4661.647585	24.201946
128.161291	4667.461733	24.206963
128.642774	4669.093012	24.211981
128.172800	4668.702636	24.216999
128.616195	4665.173755	24.222016
128.733239	4677.407625	24.227034
128.730706	4686.037418	24.232051
129.282515	4697.760855	24.237069
129.236982	4701.012780	24.242087
129.130304	4704.835869	24.247104
129.401742	4692.178131	24.252122
129.528169	4705.673937	24.257139
129.114701	4706.312083	24.262157
129.293645	4723.851451	24.267175
129.371161	4735.659980	24.272192
130.178854	4744.408698	24.277210
130.007655	4754.238522	24.282227
129.763661	4762.982670	24.287245
130.344785	4773.060266	24.292263
130.005538	4784.905805	24.297280
130.457885	4797.180434	24.302298
130.518768	4792.065405	24.307315
130.902678	4800.163263	24.312333
130.926904	4806.866522	24.317351
131.106892	4804.795406	24.322368
131.563443	4807.513572	24.327386
131.672540	4820.461909	24.332403
131.716344	4826.064226	24.337421
132.041057	4843.115435	24.342439
132.265619	4837.819004	24.347456
132.191169	4838.126707	24.352474
132.117716	4839.000428	24.357491
132.251942	4830.630516	24.362509
132.556165	4835.644885	24.367527
132.240189	4832.010718	24.372544
132.294892	4849.025048	24.377562
132.156436	4863.335681	24.382579
132.837844	4856.799890	24.387597
132.829519	4865.268129	24.392615
133.059444	4889.506049	24.397632
133.313378	4896.676152	24.402650
133.147960	4902.847753	24.407667
133.689112	4895.953991	24.412685
133.612903	4893.182622	24.417703
133.554733	4910.473562	24.422720
133.937233	4921.836533	24.427738
134.076141	4920.894717	24.432755
134.144784	4920.459038	24.437773
134.047823	4919.608562	24.442791
134.303611	4946.950017	24.447808
134.841277	4950.451325	24.452826
134.471992	4961.837358	24.457843
134.517433	4959.215575	24.462861
135.132017	4959.794103	24.467879
134.987904	4985.542911	24.472896
135.344699	4972.188505	24.477914
135.330153	4981.784696	24.482931
135.303496	4984.838270	24.487949
135.796060	4994.925132	24.492967
135.815241	5000.336289	24.497984
135.928184	5010.333513	24.503002
135.665262	5010.083337	24.508019
135.937447	5009.552994	24.513037
136.076500	5032.013879	24.518055
136.245175	5038.793376	24.523072
136.603406	5035.394638	24.528090
136.677268	5069.339755	24.533107
136.878543	5076.994668	24.538125
137.121797	5067.641176	24.543143
137.246592	5060.640928	24.548160
137.260248	5064.689911	24.553178
136.869726	5075.691707	24.558195
137.440843	5097.299335	24.563213
137.497506	5097.144395	24.568231
137.528222	5113.643640	24.573248
137.799929	5114.639492	24.578266
138.069518	5127.781664	24.583283
138.121836	5125.593794	24.588301
138.865713	5147.638736	24.593319
138.653430	5162.255174	24.598336
138.803909	5157.672515	24.603354
138.583823	5165.119904	24.608371
138.884599	5175.852804	24.613389
139.011766	5183.612149	24.618407
139.234860	5200.501390	24.623424
139.190801	5197.844350	24.628442
139.325600	5199.945217	24.633459
139.658384	5219.791438	24.638477
140.059010	5223.500117	24.643495
139.963416	5225.998933	24.648512
140.032247	5218.898402	24.653530
140.170174	5235.729700	24.658547
140.603428	5252.559466	24.663565
140.498566	5248.992296	24.668583
140.431329	5260.389665	24.673600
140.970411	5255.550622	24.678618
141.112100	5263.969877	24.683635
141.134154	5274.285074	24.688653
141.428780	5279.662233	24.693671
141.396417	5288.327998	24.698688
141.439451	5282.015245	24.703706
141.627649	5282.682354	24.708723
141.529863	5292.171217	24.713741
142.187852	5302.025807	24.718759
141.799987	5313.294285	24.723776
141.875223	5309.576071	24.728794
142.008258	5311.958374	24.733811
142.381896	5340.129556	24.738829
142.665194	5331.395340	24.743847
142.454852	5335.403839	24.748864
142.527270	5343.615662	24.753882
142.663024	5363.742681	24.758899
142.930803	5367.989935	24.763917
143.280018	5372.048125	24.768935
143.286379	5396.886038	24.773952
143.363900	5391.780663	24.778970
143.489658	5403.276182	24.783987
143.742470	5406.106082	24.789005
143.712005	5416.044970	24.794023
143.751632	5441.066453	24.799040
144.006624	5435.646669	24.804058
144.048642	5441.247927	24.809075
144.432648	5452.120431	24.814093
144.813099	5455.774619	24.819111
144.706162	5453.912264	24.824128
145.110642	5467.120631	24.829146
145.166030	5482.146733	24.834163
145.198486	5496.969921	24.839181
145.716164	5481.337456	24.844199
145.584691	5499.732621	24.849216
145.928869	5512.069394	24.854234
145.913287	5516.373748	24.859251
145.894458	5518.734715	24.864269
146.706407	5503.285915	24.869287
146.372917	5511.466066	24.874304
146.374878	5540.417216	24.879322
146.513405	5541.505190	24.884339
146.493814	5540.393048	24.889357
146.967994	5549.180402	24.894375
147.044230	5571.878057	24.899392
146.810643	5576.945701	24.904410
147.093519	5592.480446	24.909427
147.383595	5598.064791	24.914445
147.476547	5609.639907	24.919463
147.306382	5622.662614	24.924480
147.551804	5636.857760	24.929498
147.971777	5647.669333	24.934515
147.939284	5662.593185	24.939533
148.261171	5658.283670	24.944551
148.677983	5676.278959	24.949568
148.555076	5676.427342	24.954586
148.842848	5689.815438	24.959603
148.816018	5696.000282	24.964621
149.274323	5696.772797	24.969639
149.435607	5704.717733	24.974656
149.547709	5708.505309	24.979674
149.796081	5721.108504	24.984691
149.820867	5728.243615	24.989709
150.213114	5719.470314	24.994727
150.377377	5727.371062	24.999744
150.161939	5733.340203	25.004762
150.763459	5740.075261	25.009779
150.302311	5753.826166	25.014797
150.751654	5757.491486	25.019815
150.735248	5756.500472	25.024832
150.578679	5770.303441	25.029850
150.466840	5782.885091	25.034867
150.943910	5789.544658	25.039885
151.194840	5801.945106	25.044903
151.331289	5824.701298	25.049920
151.617921	5818.757582	25.054938
151.686194	5833.895292	25.059955
151.671624	5858.689750	25.064973
152.047937	5849.487849	25.069991
152.115319	5859.910918	25.075008
152.511078	5887.318303	25.080026
152.689504	5891.798605	25.085043
152.253896	5889.507368	25.090061
152.754010	5881.368606	25.095079
153.099149	5911.263873	25.100096
153.348410	5923.326457	25.105114
153.505649	5918.734585	25.110131
153.130659	5936.310535	25.115149
153.680862	5924.579110	25.120167
153.750017	5936.625788	25.125184
153.496070	5946.514131	25.130202
154.098405	5937.188599	25.135219
154.011592	5953.980233	25.140237
154.357073	5976.020907	25.145255
154.249407	5972.859998	25.150272
154.211349	5979.616969	25.155290
154.524707	5992.716017	25.160307
154.924104	6011.268587	25.165325
154.788433	6025.003356	25.170343
154.927514	6032.125627	25.175360
155.121770	6037.681073	25.180378
155.886640	6055.168434	25.185395
155.879366	6053.586828	25.190413
155.931878	6057.017351	25.195431
156.039501	6058.978708	25.200448
156.604886	6079.957055	25.205466
156.632336	6093.431825	25.210483
156.446112	6101.248133	25.215501
156.834669	6087.874145	25.220519
156.744520	6099.824811	25.225536
156.800357	6126.944241	25.230554
157.096054	6123.240596	25.235571
156.981985	6145.737026	25.240589
157.092161	6153.246865	25.245607
157.293847	6165.743153	25.250624
157.440809	6175.292912	25.255642
157.775251	6185.661440	25.260659
158.068150	6209.022359	25.265677
158.219161	6207.010582	25.270695
158.687461	6220.768580	25.275712
158.639506	6221.134146	25.280730
159.151064	6219.784169	25.285747
159.378050	6238.798636	25.290765
159.360661	6248.870952	25.295783
159.655545	6243.851453	25.300800
159.474476	6256.938701	25.305818
159.947621	6254.902830	25.310835
159.778889	6262.065041	25.315853
159.933916	6265.143971	25.320871
160.068843	6274.736732	25.325888
160.093284	6280.481767	25.330906
160.228179	6302.412002	25.335923
160.146187	6315.884570	25.340941
160.289797	6313.759023	25.345959
160.435217	6328.839968	25.350976
160.732449	6355.377296	25.355994
160.869815	6363.670276	25.361011
160.821163	6374.985842	25.366029
161.059645	6394.939703	25.371047
161.515591	6411.947709	25.376064
161.398859	6414.533684	25.381082
162.077096	6426.549796	25.386099
162.340896	6440.704044	25.391117
162.671058	6431.399175	25.396135
162.769858	6437.477711	25.401152
162.371650	6448.066699	25.406170
162.772920	6463.970216	25.411187
162.737581	6464.690459	25.416205
162.822679	6474.293937	25.421223
163.089132	6494.006253	25.426240
163.230519	6498.604286	25.431258
163.400829	6493.851792	25.436275
163.359556	6521.438422	25.441293
163.455827	6532.946729	25.446311
163.607359	6540.687758	25.451328
163.836349	6563.696707	25.456346
164.052809	6574.410242	25.461363
164.164096	6585.990924	25.466381
164.262143	6591.776677	25.471399
164.680114	6610.633243	25.476416
164.826252	6630.856252	25.481434
165.102238	6635.811684	25.486451
164.940833	6636.014869	25.491469
164.976663	6657.384695	25.496487
165.928880	6667.039539	25.501504
165.671961	6673.263573	25.506522
166.188352	6688.245764	25.511539
166.464279	6695.208691	25.516557
166.609357	6686.077588	25.521575
166.878626	6687.967426	25.526592
166.949080	6695.661286	25.531610
166.847569	6705.026396	25.536627
167.205728	6724.659270	25.541645
167.157475	6713.342348	25.546663
167.636235	6735.870039	25.551680
167.574484	6757.134052	25.556698
168.210307	6738.645237	25.561715
167.991432	6748.350299	25.566733
167.647735	6754.695023	25.571751
168.354177	6765.991637	25.576768
168.162799	6783.831555	25.581786
168.566569	6795.490860	25.586803
168.659606	6802.645503	25.591821
168.771071	6811.886493	25.596839
169.038823	6815.442279	25.601856
169.305673	6845.582228	25.606874
169.743686	6846.382574	25.611891
169.893652	6845.650673	25.616909
170.093484	6839.432276	25.621927
170.266694	6857.272678	25.626944
170.247334	6865.860378	25.631962
170.783662	6863.105976	25.636979
171.040554	6872.905767	25.641997
170.479887	6872.643322	25.647015
171.127918	6872.862402	25.652032
171.072179	6904.648211	25.657050
171.204569	6898.148750	25.662067
171.250693	6906.796533	25.667085
171.225111	6911.085200	25.672103
171.567512	6927.954227	25.677120
171.557151	6933.282331	25.682138
171.811869	6943.823621	25.687156
172.141016	6962.738603	25.692173
172.453830	6965.541942	25.697191
172.852917	6974.256664	25.702208
172.595157	6988.921295	25.707226
172.574967	6981.209745	25.712244
173.089457	7002.936475	25.717261
172.911303	7024.035791	25.722279
173.223822	7014.200312	25.727296
173.359326	7037.779062	25.732314
173.417783	7049.289270	25.737332
173.740642	7049.805441	25.742349
173.583713	7062.846840	25.747367
174.041238	7081.824235	25.752384
174.124118	7090.806276	25.757402
174.481568	7105.792289	25.762420
174.636010	7119.513153	25.767437
174.901330	7119.745070	25.772455
175.080306	7123.269916	25.777472
175.147240	7137.418730	25.782490
175.207640	7147.902481	25.787508
175.469231	7154.423790	25.792525
175.376107	7164.320974	25.797543
175.828215	7173.796507	25.802560
175.668341	7184.115059	25.807578
175.820179	7211.839529	25.812596
176.003555	7216.519832	25.817613
176.168267	7236.710623	25.822631
176.365192	7241.134307	25.827648
176.705964	7264.796040	25.832666
177.041349	7276.350441	25.837684
177.187701	7276.157035	25.842701
177.596886	7295.446682	25.847719
178.219717	7290.315173	25.852736
177.906331	7308.642090	25.857754
178.095532	7310.405832	25.862772
178.476770	7326.074109	25.867789
178.837036	7351.811183	25.872807
179.168547	7340.671276	25.877824
179.016355	7330.724940	25.882842
179.184875	7334.296454	25.887860
179.058131	7339.743947	25.892877
179.020839	7358.263153	25.897895
179.364256	7361.804987	25.902912
179.403401	7397.631383	25.907930
179.563788	7411.291663	25.912948
180.172601	7407.616318	25.917965
180.233443	7428.446710	25.922983
180.394591	7427.706635	25.928000
180.709105	7432.905619	25.933018
180.998086	7438.963358	25.938036
181.216619	7446.889872	25.943053
181.420807	7456.758592	25.948071
181.568258	7451.711879	25.953088
181.365773	7466.248106	25.958106
181.532753	7482.691486	25.963124
181.826804	7478.514458	25.968141
181.728972	7506.554781	25.973159
181.773054	7517.981858	25.978176
182.116798	7538.277344	25.983194
182.395009	7549.002606	25.988212
182.579014	7563.116707	25.993229
182.289791	7584.727369	25.998247
182.864673	7591.136451	26.003264
183.186398	7615.905280	26.008282
183.550657	7619.965119	26.013300
183.575162	7632.643068	26.018317
183.863533	7653.358977	26.023335
183.920009	7657.182207	26.028352
184.285513	7685.058866	26.033370
184.468816	7670.230469	26.038388
184.520708	7674.296253	26.043405
184.460707	7706.469516	26.048423
185.063825	7698.361640	26.053440
185.305674	7710.556383	26.058458
185.818794	7727.873772	26.063476
185.959389	7730.029943	26.068493
186.161656	7734.517467	26.073511
186.274264	7727.520019	26.078528
186.494665	7721.772803	26.083546
186.480695	7738.154199	26.088564
186.919731	7747.848042	26.093581
186.644575	7763.457450	26.098599
186.819776	7766.495538	26.103616
186.960702	7761.127676	26.108634
187.032704	7765.372885	26.113652
187.108387	7782.238066	26.118669
187.165414	7806.777633	26.123687
187.759584	7816.073348	26.128704
187.787569	7823.000558	26.133722
188.056739	7829.242871	26.138740
188.069779	7841.414087	26.143757
188.201940	7868.642831	26.148775
188.413700	7871.841872	26.153792
188.440207	7890.904849	26.158810
188.183917	7910.969161	26.163828
188.995771	7923.588136	26.168845
188.941563	7933.893655	26.173863
189.110668	7956.387620	26.178880
189.535658	7967.580386	26.183898
189.497311	7987.215764	26.188916
189.604345	7992.338951	26.193933
190.146706	8019.806561	26.198951
190.630213	8030.615585	26.203968
190.861940	8041.238596	26.208986
190.929007	8052.005389	26.214004
191.565984	8055.524869	26.219021
191.175381	8064.065867	26.224039
191.440632	8077.531395	26.229056
191.746861	8083.822818	26.234074
191.835906	8104.069752	26.239092
192.352433	8095.666448	26.244109
192.018469	8114.963319	26.249127
192.526291	8135.552237	26.254144
193.096772	8137.509841	26.259162
192.955375	8146.624841	26.264180
193.206136	8160.340147	26.269197
193.573554	8169.066280	26.274215
193.339038	8177.517752	26.279232
193.710966	8182.443645	26.284250
193.748896	8202.559740	26.289268
194.135904	8198.367954	26.294285
194.310971	8209.762074	26.299303
194.369066	8235.561543	26.304320
194.649057	8248.730209	26.309338
194.914322	8253.244491	26.314356
195.058877	8266.971137	26.319373
194.838638	8272.625792	26.324391
195.162872	8294.586585	26.329408
195.401380	8309.312212	26.334426
195.531321	8333.688534	26.339444
195.933554	8342.032522	26.344461
196.354693	8351.903763	26.349479
196.360929	8371.831552	26.354496
196.574167	8375.520360	26.359514
196.825145	8394.981630	26.364532
197.300885	8404.179117	26.369549
197.101348	8418.370743	26.374567
197.382478	8418.806431	26.379584
197.825216	8421.499565	26.384602
197.552848	8433.496279	26.389620
197.705704	8438.480504	26.394637
197.742032	8457.514185	26.399655
197.924102	8472.671464	26.404672
198.360922	8479.703117	26.409690
198.564076	8500.909952	26.414708
198.916542	8518.261056	26.419725
198.959305	8520.680032	26.424743
199.223404	8539.422557	26.429760
199.474507	8554.389713	26.434778
199.373475	8553.422744	26.439796
199.760304	8565.963598	26.444813
200.025276	8592.643921	26.449831
200.203039	8585.915733	26.454848
200.941324	8607.764440	26.459866
201.053532	8615.594902	26.464884
201.259749	8606.942508	26.469901
201.449175	8621.496953	26.474919
201.462276	8635.494534	26.479936
201.631965	8637.010391	26.484954
201.742180	8645.146803	26.489972
202.086523	8646.718870	26.494989
201.906798	8659.779526	26.500007
202.062192	8680.081607	26.505024
202.201992	8695.276014	26.510042
202.302663	8702.866616	26.515060
202.629208	8724.862281	26.520077
202.667887	8745.604337	26.525095
202.786234	8763.451230	26.530112
203.576621	8789.707957	26.535130
203.471316	8806.385952	26.540148
203.476030	8812.180065	26.545165
203.829429	8838.669756	26.550183
203.631527	8854.521883	26.555200
204.129291	8861.191553	26.560218
204.673410	8886.070557	26.565236
204.897337	8892.098646	26.570253
204.983597	8922.485850	26.575271
205.164411	8937.802889	26.580288
205.431809	8933.682660	26.585306
205.657239	8948.929325	26.590324
206.249186	8962.013960	26.595341
206.355351	8969.746349	26.600359
206.981941	8978.878290	26.605376
207.237644	8977.634170	26.610394
207.091709	9000.154101	26.615412
207.206766	9010.858479	26.620429
207.299390	8996.803137	26.625447
207.662081	9027.107060	26.630464
208.083126	9037.805009	26.635482
207.780935	9037.810146	26.640500
208.457223	9053.388068	26.645517
208.372524	9054.485998	26.650535
208.455029	9063.586584	26.655552
208.634045	9088.817668	26.660570
208.834072	9091.951944	26.665588
209.231934	9096.751752	26.670605
209.374958	9127.664798	26.675623
209.723397	9140.456629	26.680640
209.638828	9140.399029	26.685658
209.726826	9170.391796	26.690676
210.224704	9179.152858	26.695693
210.447643	9197.065664	26.700711
210.202225	9213.538809	26.705728
210.697678	9227.731327	26.710746
210.853877	9239.803558	26.715764
210.759400	9264.813873	26.720781
211.196918	9277.066503	26.725799
211.432422	9304.682353	26.730816
211.387702	9307.786220	26.735834
211.749426	9334.621156	26.740852
212.056861	9338.982273	26.745869
212.315106	9358.326160	26.750887
212.203819	9378.792137	26.755904
212.989315	9401.832998	26.760922
213.180977	9408.869339	26.765940
213.358245	9416.801297	26.770957
213.604584	9434.869617	26.775975
213.657466	9455.330623	26.780992
213.972914	9447.715228	26.786010
214.052691	9466.701192	26.791028
214.307577	9465.913242	26.796045
214.662715	9486.612642	26.801063
214.763939	9496.411427	26.806080
215.249815	9499.431602	26.811098
214.936571	9511.533553	26.816116
215.087510	9536.051611	26.821133
215.518695	9544.346554	26.826151
215.649168	9561.877263	26.831168
215.606465	9578.846622	26.836186
215.782764	9601.343305	26.841204
215.806378	9619.212326	26.846221
216.512628	9624.088161	26.851239
216.188133	9656.587917	26.856256
216.383381	9677.036713	26.861274
217.160153	9700.553644	26.866292
217.319375	9709.332358	26.871309
217.503145	9732.325031	26.876327
217.903267	9752.092582	26.881344
218.432263	9763.554586	26.886362
218.369090	9781.203392	26.891380
218.788359	9788.088866	26.896397
218.648662	9801.940211	26.901415
219.365173	9819.708364	26.906432
219.837620	9824.414938	26.911450
219.416130	9843.890627	26.916468
219.895655	9856.236016	26.921485
220.461502	9854.500259	26.926503
220.409220	9876.562473	26.931520
220.923113	9896.390965	26.936538
220.705593	9901.225739	26.941556
220.958435	9900.677571	26.946573
221.079334	9916.275636	26.951591
221.251706	9928.924685	26.956608
221.829152	9939.319340	26.961626
222.119359	9960.073409	26.966644
222.152676	9952.865163	26.971661
222.564291	9966.252973	26.976679
222.625659	9994.138255	26.981696
223.090802	9995.237566	26.986714
222.636479	10005.054407	26.991732
222.728225	10023.315146	26.996749
223.315953	10042.087108	27.001767
223.412138	10055.698833	27.006784
223.440743	10060.259824	27.011802
224.082497	10083.874466	27.016820
224.062830	10104.257702	27.021837
224.739207	10119.325429	27.026855
224.615618	10145.486493	27.031872
224.913737	10143.244323	27.036890
225.397614	10155.244991	27.041908
225.198321	10184.185896	27.046925
225.431774	10190.352333	27.051943
225.955025	10211.992226	27.056960
225.792874	10225.689315	27.061978
226.073826	10244.192386	27.066996
226.430583	10260.880632	27.072013
226.837525	10263.004173	27.077031
226.654990	10298.324688	27.082048
227.184417	10315.082928	27.087066
227.110965	10328.663833	27.092084
227.243266	10348.229027	27.097101
227.438173	10367.139535	27.102119
227.553844	10383.483329	27.107136
227.979363	10404.085642	27.112154
228.296441	10427.252650	27.117172
228.085845	10436.590715	27.122189
228.529832	10454.760664	27.127207
229.047763	10487.030754	27.132224
229.540601	10488.348456	27.137242
229.978766	10494.268499	27.142260
229.905557	10506.999543	27.147277
230.527773	10500.542148	27.152295
230.546882	10519.013965	27.157312
231.029146	10515.922070	27.162330
231.278534	10530.529010	27.167348
231.350798	10547.819131	27.172365
231.473062	10553.059577	27.177383
230.996592	10563.505884	27.182400
231.824575	10570.850383	27.187418
231.978179	10589.280366	27.192436
232.281428	10609.143761	27.197453
232.472331	10606.507253	27.202471
232.920231	10637.926638	27.207488
233.150907	10644.964171	27.212506
233.466989	10643.790301	27.217524
233.508983	10666.867614	27.222541
233.531434	10683.470530	27.227559
233.556568	10699.681509	27.232576
233.811790	10712.322217	27.237594
234.276385	10726.433734	27.242612
234.153939	10742.072024	27.247629
234.423335	10768.047861	27.252647
234.407185	10796.672082	27.257664
234.717205	10816.343192	27.262682
234.987123	10837.695721	27.267700
234.989951	10870.618876	27.272717
235.569808	10883.181663	27.277735
235.654914	10908.481557	27.282752
235.902121	10930.875442	27.287770
236.700685	10938.283269	27.292788
236.764008	10964.333647	27.297805
237.304159	10987.409468	27.302823
237.414892	10996.075585	27.307840
237.794230	11015.953699	27.312858
238.194072	11027.279615	27.317876
238.202141	11035.655488	27.322893
238.541772	11045.280338	27.327911
238.975864	11059.964382	27.332928
238.829996	11079.469293	27.337946
239.301635	11081.972990	27.342964
239.077291	11112.600018	27.347981
239.354842	11115.373694	27.352999
239.273468	11139.671843	27.358016
239.665168	11154.399216	27.363034
240.103851	11173.147508	27.368052
240.475115	11208.302114	27.373069
240.743146	11212.249589	27.378087
240.882557	11227.767885	27.383104
241.066201	11255.465790	27.388122
241.538275	11267.539360	27.393140
241.656544	11287.308116	27.398157
241.753333	11302.894186	27.403175
242.242826	11317.481082	27.408192
242.237388	11329.397259	27.413210
242.498275	11350.402190	27.418228
242.266827	11382.685246	27.423245
242.481196	11392.255374	27.428263
243.042997	11429.821114	27.433280
243.053014	11457.123437	27.438298
243.446453	11464.438525	27.443316
243.681799	11497.637301	27.448333
244.370082	11519.379322	27.453351
244.407869	11530.633853	27.458368
244.713480	11546.954542	27.463386
244.681540	11567.088785	27.468404
244.915712	11577.638129	27.473421
245.310792	11583.430985	27.478439
245.850743	11609.726658	27.483456
245.980884	11624.606393	27.488474
246.315815	11633.553295	27.493492
246.264514	11655.557135	27.498509
246.475320	11661.592383	27.503527
246.760578	11681.929608	27.508544
246.846284	11708.725904	27.513562
247.137741	11720.947828	27.518580
246.978275	11758.332565	27.523597
247.634032	11757.041049	27.528615
247.900191	11796.737865	27.533632
247.966887	11819.762334	27.538650
248.284831	11834.333140	27.543668
248.607120	11866.114444	27.548685
248.973800	11892.916619	27.553703
249.241183	11903.296038	27.558720
249.668581	11914.911096	27.563738
249.772773	11943.083394	27.568756
250.129977	11974.344703	27.573773
250.131296	11990.875256	27.578791
250.538141	12005.529218	27.583808
250.591198	12022.393166	27.588826
251.039719	12045.444685	27.593844
251.171237	12067.506329	27.598861
251.447384	12086.489740	27.603879
252.016202	12111.397271	27.608896
252.232285	12128.451834	27.613914
252.886599	12141.673745	27.618932
252.950430	12155.788925	27.623949
253.416961	12173.120436	27.628967
253.856518	12169.682345	27.633984
253.865168	12188.199563	27.639002
254.271423	12193.701665	27.644020
254.489990	12206.677343	27.649037
254.875173	12214.566099	27.654055
255.200603	12224.042744	27.659072
255.090129	12244.356251	27.664090
255.277843	12247.869768	27.669108
255.462157	12274.100024	27.674125
255.635170	12280.085813	27.679143
255.958128	12302.412373	27.684160
255.725724	12317.753653	27.689178
256.490154	12330.394230	27.694196
256.454487	12359.687810	27.699213
256.692311	12380.698686	27.704231
257.229970	12392.640157	27.709248
257.148214	12423.734574	27.714266
257.723016	12446.952521	27.719284
257.621157	12452.453576	27.724301
257.818075	12491.370194	27.729319
258.190189	12508.853175	27.734336
258.042072	12534.456509	27.739354
258.633776	12555.544655	27.744372
258.855048	12575.290885	27.749389
258.938434	12602.418367	27.754407
259.372902	12629.231054	27.759424
259.348469	12660.027316	27.764442
259.928637	12674.966817	27.769460
260.218778	12695.287972	27.774477
260.826503	12714.631750	27.779495
261.358962	12721.057813	27.784512
261.348304	12743.757607	27.789530
261.825572	12758.432136	27.794548
261.563174	12760.437340	27.799565
261.591662	12790.259203	27.804583
261.761275	12804.281839	27.809600
262.007856	12825.610929	27.814618
262.603620	12845.201074	27.819636
263.127604	12867.990766	27.824653
263.309940	12879.346839	27.829671
263.939632	12891.615405	27.834688
263.864908	12912.849578	27.839706
264.158778	12924.179376	27.844724
264.400526	12941.817514	27.849741
264.632813	12964.529478	27.854759
265.103998	12977.894213	27.859776
265.043151	12995.509920	27.864794
265.351124	13011.985340	27.869812
265.542642	13033.867427	27.874829
265.636892	13059.233795	27.879847
266.058553	13076.891204	27.884864
266.002972	13091.799040	27.889882
266.445453	13117.839106	27.894900
266.982469	13139.427895	27.899917
266.792328	13159.063176	27.904935
267.420412	13187.522966	27.909952
267.373102	13218.164920	27.914970
267.788756	13236.307250	27.919988
268.019015	13266.091926	27.925005
268.362526	13283.508777	27.930023
268.746445	13303.263692	27.935040
268.849223	13332.322646	27.940058
269.215762	13348.229339	27.945076
269.753179	13367.787215	27.950093
270.011669	13391.374724	27.955111
270.607857	13413.401620	27.960128
270.715555	13424.307132	27.965146
271.026835	13430.357173	27.970164
271.095830	13443.048132	27.975181
271.555689	13472.325677	27.980199
271.727850	13485.217081	27.985216
271.716971	13509.211693	27.990234
272.009289	13521.794907	27.995252
272.814213	13553.532102	28.000269
272.758646	13565.060327	28.005287
273.137058	13587.745873	28.010304
273.458702	13607.966850	28.015322
273.757917	13625.597817	28.020340
273.880280	13643.193413	28.025357
274.017513	13663.493776	28.030375
274.523456	13675.025433	28.035392
274.555780	13716.610066	28.040410
274.837843	13731.163304	28.045428
275.129392	13738.055044	28.050445
275.270881	13780.337216	28.055463
275.695388	13797.235407	28.060480
275.693129	13820.305635	28.065498
276.118615	13848.659816	28.070516
276.215495	13855.038538	28.075533
276.410033	13892.329536	28.080551
276.629037	13909.001787	28.085568
277.153949	13936.205110	28.090586
277.426222	13959.211268	28.095604
277.701490	13978.000073	28.100621
278.102056	14002.274117	28.105639
278.557737	14028.488386	28.110656
278.885841	14053.951620	28.115674
279.283231	14062.917134	28.120692
279.793333	14080.310472	28.125709
279.720432	14106.760325	28.130727
280.396260	14107.357898	28.135744
280.661248	14119.689233	28.140762
280.797908	14137.832970	28.145780
281.082563	14151.191676	28.150797
280.976732	14157.260476	28.155815
281.270228	14176.869086	28.160832
281.398498	14203.892558	28.165850
281.848428	14213.919472	28.170868
282.007125	14225.986373	28.175885
282.216408	14257.719353	28.180903
282.751171	14277.849226	28.185920
282.993598	14287.475534	28.190938
283.209440	14305.757658	28.195956
283.528050	14319.585224	28.200973
283.822729	14338.368088	28.205991
284.089235	14357.032711	28.211008
284.342851	14386.284524	28.216026
284.424734	14401.498629	28.221044
284.821279	14413.042585	28.226061
284.689380	14444.548641	28.231079
285.058197	14464.725073	28.236096
285.413358	14498.246668	28.241114
285.567804	14521.392856	28.246132
286.159756	14545.292554	28.251149
286.412004	14564.482962	28.256167
286.882168	14600.256604	28.261184
287.239252	14624.641196	28.266202
287.410360	14652.411607	28.271220
287.691371	14676.421177	28.276237
287.566550	14689.852704	28.281255
288.109595	14719.823182	28.286272
288.491736	14745.540171	28.291290
288.175203	14771.044843	28.296308
289.044897	14808.429689	28.301325
288.741461	14834.693456	28.306343
289.462083	14856.763220	28.311360
289.789663	14893.437266	28.316378
290.046191	14925.159014	28.321396
290.053511	14934.038168	28.326413
290.395980	14974.827794	28.331431
291.117665	14992.743455	28.336448
291.667918	15012.131000	28.341466
291.918954	15044.512622	28.346484
292.262542	15054.702611	28.351501
292.367159	15090.424257	28.356519
292.658549	15116.771437	28.361536
292.974900	15136.286025	28.366554
293.285356	15158.025252	28.371572
293.930440	15180.851777	28.376589
294.061963	15197.372755	28.381607
294.589092	15216.510638	28.386624
294.747052	15240.256124	28.391642
294.796589	15265.036041	28.396660
295.154962	15274.557102	28.401677
295.258813	15316.234863	28.406695
295.875253	15319.858668	28.411712
296.196410	15342.324462	28.416730
296.388248	15360.904864	28.421748
297.246882	15375.340683	28.426765
297.064973	15412.003935	28.431783
297.542606	15412.388462	28.436800
297.906114	15437.939420	28.441818
297.701647	15460.541069	28.446836
298.436042	15471.388546	28.451853
298.089183	15481.796886	28.456871
298.525663	15513.231590	28.461888
298.748371	15534.560305	28.466906
298.760220	15565.969130	28.471924
299.394661	15585.307203	28.476941
299.415554	15619.943808	28.481959
299.665051	15639.342390	28.486976
300.211857	15666.393699	28.491994
300.219535	15703.642492	28.497012
300.632953	15722.107898	28.502029
301.040342	15749.869510	28.507047
301.200232	15773.416877	28.512064
301.486143	15804.735178	28.517082
301.477275	15828.877864	28.522100
302.031976	15861.067521	28.527117
302.022093	15900.645840	28.532135
302.321028	15922.616510	28.537152
302.836466	15947.689276	28.542170
303.188630	15981.181318	28.547188
303.611544	16012.107019	28.552205
303.829266	16042.280245	28.557223
304.449167	16054.125735	28.562240
304.855423	16083.300214	28.567258
305.376084	16124.113705	28.572276
305.532806	16130.103611	28.577293
305.787066	16169.456121	28.582311
306.351284	16184.054775	28.587328
306.645095	16205.654729	28.592346
306.815767	16226.132428	28.597364
307.158389	16243.426518	28.602381
307.509505	16275.006026	28.607399
307.919550	16297.811482	28.612416
308.335622	16308.612819	28.617434
308.460346	16332.737329	28.622452
309.137863	16341.339464	28.627469
309.313546	16370.524179	28.632487
309.605642	16385.944963	28.637504
310.098954	16404.322293	28.642522
309.888026	16426.149345	28.647540
310.478453	16443.230917	28.652557
310.715131	16467.542017	28.657575
310.923488	16493.388187	28.662592
311.091197	16512.932130	28.667610
311.031444	16545.643881	28.672628
311.700786	16562.175102	28.677645
311.895772	16585.120508	28.682663
312.129407	16625.386913	28.687680
312.474176	16654.459090	28.692698
312.755656	16678.785167	28.697716
313.225283	16703.510466	28.702733
313.623778	16746.553782	28.707751
313.471886	16772.538712	28.712768
313.818263	16801.417025	28.717786
314.367560	16835.790803	28.722804
314.646494	16851.838334	28.727821
314.952056	16882.495065	28.732839
315.132072	16918.224001	28.737856
315.788467	16943.375877	28.742874
316.083763	16971.857870	28.747892
316.458363	17003.830504	28.752909
316.665806	17033.151423	28.757927
316.992526	17050.928131	28.762944
317.511395	17085.252295	28.767962
317.386536	17113.406764	28.772980
318.055548	17134.630731	28.777997
318.471380	17175.388504	28.783015
318.600302	17198.118719	28.788032
318.924709	17206.625189	28.793050
319.045502	17248.063913	28.798068
319.468889	17272.745697	28.803085
320.012162	17305.890493	28.808103
320.056296	17328.806694	28.813120
320.781653	17351.424400	28.818138
320.947151	17380.726074	28.823156
321.334271	17390.071822	28.828173
321.616987	17414.627325	28.833191
321.602090	17447.746409	28.838208
322.072832	17456.763150	28.843226
322.194880	17490.551627	28.848244
322.372814	17508.041331	28.853261
322.709058	17540.481584	28.858279
323.024317	17571.486329	28.863296
323.683064	17598.076282	28.868314
323.686874	17622.022486	28.873332
324.289229	17641.398242	28.878349
324.920973	17688.298633	28.883367
324.810564	17705.256150	28.888384
325.522381	17726.054549	28.893402
325.533617	17762.234040	28.898420
325.832508	17784.659575	28.903437
326.572430	17803.781097	28.908455
326.606831	17828.187521	28.913472
326.985352	17845.950227	28.918490
326.954002	17882.589384	28.923508
327.108517	17912.565276	28.928525
327.092421	17946.223041	28.933543
327.607032	17990.724175	28.938560
328.073331	18017.523135	28.943578
328.441832	18056.705244	28.948596
329.304492	18083.990505	28.953613
329.590648	18113.259361	28.958631
329.573176	18163.381385	28.963648
330.392145	18179.869030	28.968666
330.510792	18211.791721	28.973684
331.124196	18235.715341	28.978701
331.261894	18272.485057	28.983719
331.570744	18290.221922	28.988736
332.111815	18315.743299	28.993754
332.061571	18357.684359	28.998772
332.249001	18373.745339	29.003789
332.882690	18403.529471	29.008807
333.271704	18443.122083	29.013824
333.506339	18468.823574	29.018842
333.689898	18510.403263	29.023860
334.258615	18537.345350	29.028877
334.648380	18557.111964	29.033895
334.838579	18592.787675	29.038912
335.232324	18624.580597	29.043930
335.480486	18651.998267	29.048948
336.098432	18680.571773	29.053965
336.354192	18705.428413	29.058983
337.091676	18734.228162	29.064000
337.457669	18754.714569	29.069018
337.707344	18783.041718	29.074036
338.165276	18805.785996	29.079053
338.265542	18815.561406	29.084071
338.494862	18852.203781	29.089088
338.740660	18879.697880	29.094106
338.978199	18911.556566	29.099124
339.155022	18939.866069	29.104141
339.805953	18965.616204	29.109159
340.242478	18996.840035	29.114176
340.516801	19035.121037	29.119194
340.629973	19060.654356	29.124212
341.008379	19066.499946	29.129229
341.751293	19100.526472	29.134247
341.779198	19129.989540	29.139264
342.417106	19154.715941	29.144282
342.707222	19182.816409	29.149300
343.052428	19209.572679	29.154317
343.763048	19218.087322	29.159335
343.643608	19255.899512	29.164352
343.883808	19259.293171	29.169370
343.906850	19289.734648	29.174388
343.969180	19319.605363	29.179405
344.352412	19347.230437	29.184423
344.583712	19384.401731	29.189440
344.838840	19417.267339	29.194458
345.421607	19453.179553	29.199476
345.733599	19489.205936	29.204493
346.129868	19506.671144	29.209511
346.446540	19553.184346	29.214528
346.764472	19576.539214	29.219546
347.181143	19602.401553	29.224564
347.501503	19641.094081	29.229581
348.179453	19673.414283	29.234599
348.230287	19710.001337	29.239616
348.691479	19733.285468	29.244634
348.977551	19765.613840	29.249652
349.448854	19810.331948	29.254669
350.033841	19840.988992	29.259687
349.966658	19868.645205	29.264704
350.483208	19895.144122	29.269722
351.314192	19931.295384	29.274740
351.368414	19953.165250	29.279757
352.186124	19980.355455	29.284775
351.891323	20013.661474	29.289792
352.463253	20040.148321	29.294810
353.133293	20077.773625	29.299828
352.884486	20115.848751	29.304845
353.678273	20126.568131	29.309863
353.587235	20172.470986	29.314880
354.168513	20199.662775	29.319898
354.413069	20238.343993	29.324916
354.831731	20270.009837	29.329933
355.354646	20304.305336	29.334951
355.342040	20344.181648	29.339968
355.651612	20379.590823	29.344986
356.033188	20403.216943	29.350004
356.440744	20446.922611	29.355021
357.050399	20480.989748	29.360039
356.831192	20510.481892	29.365056
357.605103	20553.901886	29.370074
358.387257	20590.751558	29.375092
358.745410	20619.834801	29.380109
359.414748	20644.982298	29.385127
359.313901	20686.887141	29.390144
359.621635	20714.388229	29.395162
359.926879	20733.198722	29.400180
359.925645	20764.154522	29.405197
360.796056	20796.412007	29.410215
361.168258	20838.893318	29.415232
361.657115	20856.751380	29.420250
361.879512	20885.561135	29.425268
362.163251	20925.136064	29.430285
362.457518	20958.188999	29.435303
362.982393	20989.394095	29.440320
363.472328	21017.611263	29.445338
363.897268	21039.321990	29.450356
363.844462	21087.855362	29.455373
364.494490	21105.058042	29.460391
364.771376	21136.968087	29.465408
364.774298	21181.601716	29.470426
365.094260	21210.566177	29.475444
365.179565	21252.304525	29.480461
366.028132	21292.773911	29.485479
366.407645	21326.754673	29.490496
366.584652	21363.304009	29.495514
366.920557	21395.444428	29.500532
367.223609	21429.901530	29.505549
367.433209	21451.906918	29.510567
367.566682	21493.374628	29.515584
368.171405	21530.506356	29.520602
368.742041	21556.486604	29.525620
368.929544	21600.148082	29.530637
369.276875	21632.883004	29.535655
369.272633	21669.675783	29.540672
369.856547	21712.777030	29.545690
370.397722	21747.608505	29.550708
370.580144	21789.863447	29.555725
371.296725	21816.696559	29.560743
371.541511	21859.546776	29.565760
372.062558	21904.427814	29.570778
372.734388	21925.725257	29.575796
373.454021	21940.276535	29.580813
374.420955	21971.823499	29.585831
374.421559	22010.385148	29.590848
374.544201	22018.413461	29.595866
374.848177	22053.092412	29.600884
374.983659	22090.728579	29.605901
375.608641	22111.270927	29.610919
375.858810	22147.573395	29.615936
376.075383	22176.450973	29.620954
376.459083	22207.161382	29.625972
376.429010	22254.806743	29.630989
377.053009	22297.462997	29.636007
377.555249	22328.997534	29.641024
377.766968	22357.880954	29.646042
378.436620	22403.448254	29.651060
378.565388	22434.481832	29.656077
379.217086	22456.596815	29.661095
379.487762	22496.357344	29.666112
379.880728	22532.219245	29.671130
380.385669	22562.711620	29.676148
380.573959	22590.501971	29.681165
381.035603	22617.878276	29.686183
381.584743	22656.361825	29.691200
381.739791	22690.730868	29.696218
382.500842	22731.287560	29.701236
382.914393	22769.052738	29.706253
383.271201	22796.583822	29.711271
383.591238	22821.817524	29.716288
384.248074	22857.275473	29.721306
384.823188	22876.076900	29.726324
384.968327	22910.123235	29.731341
385.330775	22940.144759	29.736359
385.827749	22963.395948	29.741376
386.554347	22990.338076	29.746394
386.211710	23025.874771	29.751412
386.347208	23060.946268	29.756429
386.830814	23085.757597	29.761447
387.375668	23125.970974	29.766464
387.440907	23159.617918	29.771482
387.917170	23182.934322	29.776500
387.981041	23231.921304	29.781517
388.665641	23265.135035	29.786535
389.044327	23302.369513	29.791552
389.239855	23343.024253	29.796570
390.184100	23387.675359	29.801588
390.038635	23442.504569	29.806605
390.083952	23464.145548	29.811623
390.925250	23509.277538	29.816640
391.451511	23550.991311	29.821658
391.879417	23573.915756	29.826676
392.310628	23615.008389	29.831693
392.597911	23665.924332	29.836711
393.163613	23694.237547	29.841728
393.392145	23715.260457	29.846746
393.892764	23746.293357	29.851764
394.080165	23777.854235	29.856781
394.281124	23804.695288	29.861799
394.832434	23846.832953	29.866816
395.016608	23886.801834	29.871834
395.881512	23918.902257	29.876852
396.068949	23959.201889	29.881869
396.669923	23992.749374	29.886887
397.103579	24022.166617	29.891904
397.210452	24067.061916	29.896922
397.362485	24083.809088	29.901940
397.435315	24128.818972	29.906957
397.767857	24173.508558	29.911975
398.231595	24215.051389	29.916992
398.763332	24270.562954	29.922010
399.353432	24312.771057	29.927028
399.486901	24346.620378	29.932045
399.907302	24401.887438	29.937063
400.470340	24439.551237	29.942080
400.701122	24489.947602	29.947098
401.405249	24526.744691	29.952116
401.816519	24571.398667	29.957133
402.660848	24593.333261	29.962151
403.601426	24633.752913	29.967168
403.631119	24675.396956	29.972186
404.157658	24695.018929	29.977204
404.716011	24732.931717	29.982221
404.684596	24761.353242	29.987239
405.374752	24779.384059	29.992256
405.825176	24832.023693	29.997274
406.048705	24849.786339	30.002292
406.612590	24889.876192	30.007309
407.052375	24932.266776	30.012327
407.487414	24960.111715	30.017344
407.437848	24997.012253	30.022362
407.926291	25045.283088	30.027380
407.775018	25085.076824	30.032397
407.981780	25129.687206	30.037415
408.711830	25172.970257	30.042432
408.781758	25221.269727	30.047450
409.386778	25272.576372	30.052468
409.845617	25319.996625	30.057485
410.200073	25371.005926	30.062503
410.838631	25417.221973	30.067520
410.977837	25473.565529	30.072538
411.344851	25517.858726	30.077556
411.868630	25557.046899	30.082573
412.095671	25602.749546	30.087591
412.927768	25645.056597	30.092608
413.353382	25690.403408	30.097626
413.728690	25734.607489	30.102644
414.376076	25771.626380	30.107661
414.771823	25823.549565	30.112679
415.483899	25859.266446	30.117696
415.792197	25899.509707	30.122714
416.080247	25936.384888	30.127732
416.402998	25977.748733	30.132749
417.057107	26013.229508	30.137767
417.482512	26053.955259	30.142784
417.602808	26095.002746	30.147802
418.012865	26139.323561	30.152820
418.278773	26177.303643	30.157837
418.696359	26231.479529	30.162855
419.372066	26264.462481	30.167872
419.432891	26315.534146	30.172890
420.105379	26353.239294	30.177908
420.394650	26396.748078	30.182925
420.642331	26451.962004	30.187943
421.305442	26482.941518	30.192960
421.304650	26525.066628	30.197978
422.017927	26575.633884	30.202996
422.631310	26604.757810	30.208013
422.542209	26656.318897	30.213031
423.513078	26696.741598	30.218048
424.097438	26732.601257	30.223066
424.554356	26761.416967	30.228084
424.950742	26806.019323	30.233101
425.212667	26847.814807	30.238119
425.787726	26875.396878	30.243136
426.081572	26924.939988	30.248154
426.661664	26963.604814	30.253172
426.988760	26996.981099	30.258189
427.307917	27046.384752	30.263207
427.779309	27077.583106	30.268224
428.088075	27126.906700	30.273242
428.537644	27169.592973	30.278260
428.841233	27201.185149	30.283277
429.232693	27247.672482	30.288295
430.044578	27290.526304	30.293312
430.324266	27326.683558	30.298330
430.974614	27374.185110	30.303348
431.161264	27412.550056	30.308365
431.533983	27461.703184	30.313383
432.319250	27489.753034	30.318400
432.482706	27544.239996	30.323418
432.930858	27581.098575	30.328436
433.307641	27634.812502	30.333453
433.966241	27682.938078	30.338471
434.192120	27721.341391	30.343488
434.530714	27771.213895	30.348506
434.932916	27822.549068	30.353524
435.593958	27863.309583	30.358541
435.662898	27907.215019	30.363559
436.424558	27964.348700	30.368576
436.393280	28014.620513	30.373594
436.979753	28050.069363	30.378612
437.627246	28097.942436	30.383629
437.618130	28155.241924	30.388647
438.647277	28199.749677	30.393664
439.022377	28254.755927	30.398682
439.209384	28301.869737	30.403700
439.626838	28336.350327	30.408717
440.015998	28404.908933	30.413735
440.370864	28459.723608	30.418752
441.092758	28506.320625	30.423770
441.566281	28546.344065	30.428788
441.944654	28600.559126	30.433805
442.555942	28655.836767	30.438823
442.967805	28685.852352	30.443840
443.726611	28740.490787	30.448858
443.753754	28782.023766	30.453876
444.399883	28824.492404	30.458893
445.071636	28884.735323	30.463911
445.324457	28924.231450	30.468928
445.642243	28966.499163	30.473946
445.938290	29024.120189	30.478964
446.257565	29066.211249	30.483981
446.734483	29121.739697	30.488999
447.241728	29169.531654	30.494016
447.485094	29215.206499	30.499034
447.724550	29278.635688	30.504052
448.551233	29330.391014	30.509069
448.988866	29379.103549	30.514087
449.708760	29421.116677	30.519104
450.001827	29479.427395	30.524122
450.403343	29524.830877	30.529140
451.367150	29561.823013	30.534157
451.512896	29613.918795	30.539175
451.658949	29637.251237	30.544192
452.518707	29687.528979	30.549210
452.715669	29735.894257	30.554228
453.130648	29764.747152	30.559245
453.291951	29819.815768	30.564263
454.191182	29868.658477	30.569280
454.623390	29913.143064	30.574298
455.230359	29960.012193	30.579316
455.688431	29996.170798	30.584333
456.192849	30035.820326	30.589351
456.293128	30083.265609	30.594368
456.848733	30136.497177	30.599386
457.067580	30178.894598	30.604404
457.610686	30234.920419	30.609421
457.998010	30288.905827	30.614439
458.471038	30331.037648	30.619456
458.895303	30385.976285	30.624474
459.501650	30435.411577	30.629492
460.065204	30484.453428	30.634509
460.608788	30533.855200	30.639527
460.757054	30589.023042	30.644544
461.466295	30631.589783	30.649562
461.647751	30678.524824	30.654580
462.004453	30732.715415	30.659597
462.393559	30801.766167	30.664615
463.241605	30842.856140	30.669632
463.680661	30894.752714	30.674650
464.281181	30946.969800	30.679668
465.089379	30993.606562	30.684685
465.270926	31057.039171	30.689703
466.005083	31084.910855	30.694720
466.708442	31138.184171	30.699738
466.748147	31192.835526	30.704756
467.444471	31218.716649	30.709773
467.720352	31283.134586	30.714791
468.066764	31329.750723	30.719808
468.579154	31372.093087	30.724826
469.063940	31436.275166	30.729844
469.621152	31471.792629	30.734861
469.875413	31530.757059	30.739879
469.924583	31584.660356	30.744896
470.718689	31639.901504	30.749914
470.915537	31703.188796	30.754932
471.734188	31755.306010	30.759949
471.880605	31817.614544	30.764967
472.253739	31874.607567	30.769984
472.817259	31923.931099	30.775002
473.288875	31992.897199	30.780020
473.754054	32040.435797	30.785037
474.165343	32102.789930	30.790055
474.694355	32178.183518	30.795072
475.591261	32223.218767	30.800090
475.905423	32274.433328	30.805108
476.628130	32313.651275	30.810125
476.918888	32385.617699	30.815143
477.042959	32435.258196	30.820160
477.779662	32484.141380	30.825178
478.735469	32544.861143	30.830196
479.470041	32588.349749	30.835213
479.727038	32634.400425	30.840231
479.973647	32687.236454	30.845248
480.552487	32731.461041	30.850266
480.675278	32793.600245	30.855284
481.420811	32841.763591	30.860301
481.709806	32899.464811	30.865319
481.946408	32938.524656	30.870336
482.606563	32995.962952	30.875354
482.838913	33044.505052	30.880372
483.363286	33090.673669	30.885389
483.905460	33161.207133	30.890407
484.159539	33215.050020	30.895424
484.889057	33256.319837	30.900442
485.175716	33319.172145	30.905460
485.717141	33362.704033	30.910477
486.473183	33423.447202	30.915495
486.550014	33476.231599	30.920512
487.052673	33527.014787	30.925530
487.375446	33583.930155	30.930548
488.092588	33656.607531	30.935565
488.545414	33711.419331	30.940583
488.978864	33776.558702	30.945600
489.886586	33841.632594	30.950618
490.025075	33895.673344	30.955636
490.567989	33948.331675	30.960653
491.139398	34010.271681	30.965671
491.322581	34069.521390	30.970688
492.056680	34137.805665	30.975706
492.654912	34206.131577	30.980724
493.222938	34254.978109	30.985741
493.930741	34313.381525	30.990759
494.080627	34378.787670	30.995776
494.821059	34420.383412	31.000794
495.168943	34491.894588	31.005812
495.811638	34549.643737	31.010829
496.371726	34600.780239	31.015847
496.782489	34664.506658	31.020864
497.163392	34716.061213	31.025882
497.524492	34788.025787	31.030900
497.956114	34855.176316	31.035917
498.404019	34911.731322	31.040935
498.634168	34977.561873	31.045952
499.317186	35055.163779	31.050970
499.800789	35122.729574	31.055988
500.580189	35179.533609	31.061005
501.116272	35253.793660	31.066023
501.569566	35310.033483	31.071040
502.545356	35369.645718	31.076058
502.450614	35443.307057	31.081076
502.998747	35494.681617	31.086093
503.178762	35566.751826	31.091111
504.008765	35635.994792	31.096128
504.952099	35686.269574	31.101146
505.449443	35757.833723	31.106164
506.161345	35809.952124	31.111181
506.754896	35865.782383	31.116199
506.840082	35926.401933	31.121216
507.532320	35985.293072	31.126234
508.078907	36046.714105	31.131252
508.430481	36093.010587	31.136269
508.872789	36164.490782	31.141287
509.297449	36232.483914	31.146304
510.060289	36288.060314	31.151322
510.400053	36361.694687	31.156340
511.003841	36412.115959	31.161357
511.787563	36468.535221	31.166375
512.119139	36540.025738	31.171392
512.903006	36577.519949	31.176410
513.428162	36639.773380	31.181428
513.846119	36700.668789	31.186445
514.673668	36749.084809	31.191463
514.942282	36803.699859	31.196480
515.726959	36863.979819	31.201498
515.824602	36918.052245	31.206516
516.032636	36959.372613	31.211533
516.705584	37028.359724	31.216551
516.706111	37085.465729	31.221568
517.443463	37133.490573	31.226586
517.686711	37203.035341	31.231604
518.139983	37247.869436	31.236621
518.968987	37320.988257	31.241639
519.552153	37380.952926	31.246656
519.978234	37436.923042	31.251674
520.294384	37503.184191	31.256692
520.840492	37557.244426	31.261709
521.472944	37632.277945	31.266727
522.054806	37696.952634	31.271744
522.423844	37749.947558	31.276762
522.913694	37822.237593	31.281780
523.610783	37884.605799	31.286797
524.062978	37936.536574	31.291815
524.258108	37997.908713	31.296832
525.391207	38071.800930	31.301850
525.558676	38149.971643	31.306868
526.121602	38205.451284	31.311885
526.507276	38269.567084	31.316903
526.581654	38351.544533	31.321920
527.412982	38411.133933	31.326938
528.536258	38484.587604	31.331956
528.714237	38549.401492	31.336973
529.274330	38612.230390	31.341991
529.823206	38695.737514	31.347008
530.426241	38756.533549	31.352026
530.886111	38830.139230	31.357044
531.155507	38904.572039	31.362061
531.968666	38964.213606	31.367079
532.192013	39041.716128	31.372096
533.137762	39125.061834	31.377114
533.612341	39189.671207	31.382132
533.888556	39264.176958	31.387149
534.907137	39341.805070	31.392167
535.203843	39401.744851	31.397184
536.169424	39464.348754	31.402202
536.861057	39542.113790	31.407220
537.703940	39598.517293	31.412237
538.041413	39650.446680	31.417255
538.336982	39707.960425	31.422272
538.991187	39774.142482	31.427290
539.363356	39849.013544	31.432308
540.255295	39896.057502	31.437325
540.640321	39966.650012	31.442343
540.986474	40028.474377	31.447360
541.872399	40092.643403	31.452378
542.289621	40164.692788	31.457396
542.714978	40231.936994	31.462413
543.434097	40283.139137	31.467431
543.768181	40350.622965	31.472448
544.541877	40417.365257	31.477466
544.985170	40485.759552	31.482484
545.498510	40542.728609	31.487501
546.513007	40604.583422	31.492519
546.466340	40662.655433	31.497536
547.044488	40738.862900	31.502554
547.689957	40804.579816	31.507572
547.982322	40859.458844	31.512589
548.917187	40930.968051	31.517607
549.149878	41007.953397	31.522624
549.874720	41059.330384	31.527642
550.234111	41140.165343	31.532660
550.799467	41209.220853	31.537677
551.655681	41267.297170	31.542695
551.928179	41329.251738	31.547712
552.522270	41381.655037	31.552730
553.049131	41436.736968	31.557748
553.184541	41512.664079	31.562765
553.988835	41567.034519	31.567783
554.244728	41636.717269	31.572800
555.033408	41696.835856	31.577818
555.510120	41767.918931	31.582836
555.738147	41832.310056	31.587853
556.347987	41908.390882	31.592871
556.929171	41979.896308	31.597888
557.590531	42042.079473	31.602906
558.131008	42109.513590	31.607924
558.622298	42184.762811	31.612941
559.704398	42263.671349	31.617959
560.263250	42327.116189	31.622976
560.993216	42386.006102	31.627994
561.528353	42455.150207	31.633012
561.974170	42522.677235	31.638029
562.748976	42583.397657	31.643047
562.822269	42649.622918	31.648064
563.399564	42722.899716	31.653082
564.341562	42788.221184	31.658100
564.601338	42855.729649	31.663117
565.373193	42930.222113	31.668135
565.555942	42995.723386	31.673152
566.243606	43065.627503	31.678170
566.781754	43139.998409	31.683188
567.155238	43214.106371	31.688205
568.195416	43287.504688	31.693223
568.266772	43369.309369	31.698240
568.984780	43431.336327	31.703258
569.349103	43510.214057	31.708276
569.566377	43590.293981	31.713293
570.537915	43660.036648	31.718311
571.393404	43741.457738	31.723328
571.875621	43819.158672	31.728346
572.661501	43894.056804	31.733364
573.014686	43972.704717	31.738381
574.065350	44038.274692	31.743399
574.393216	44111.607656	31.748416
574.916012	44179.042770	31.753434
575.614487	44265.271984	31.758452
575.783018	44339.538263	31.763469
576.460081	44392.773055	31.768487
577.522752	44478.267471	31.773504
577.849378	44552.691605	31.778522
578.854502	44606.027527	31.783540
579.412143	44691.094868	31.788557
579.990058	44739.368102	31.793575
580.805492	44824.434518	31.798592
581.310914	44894.066216	31.803610
582.170713	44953.687962	31.808628
582.252027	45020.261335	31.813645
582.723505	45089.807809	31.818663
583.278846	45167.341273	31.823680
583.937063	45236.538564	31.828698
584.429869	45305.940242	31.833716
584.798813	45376.597150	31.838733
585.537348	45448.443590	31.843751
585.936378	45524.403580	31.848768
586.479922	45599.667491	31.853786
587.208530	45682.087337	31.858804
587.745449	45763.876153	31.863821
588.305995	45833.713793	31.868839
588.807356	45913.857814	31.873856
589.494120	45981.764920	31.878874
590.610281	46050.359138	31.883892
590.779587	46126.681572	31.888909
591.159578	46195.666293	31.893927
591.989139	46252.859615	31.898944
592.546846	46320.779792	31.903962
593.179455	46394.914435	31.908980
593.429007	46454.632286	31.913997
593.973785	46531.109059	31.919015
594.493937	46605.695689	31.924032
595.115085	46676.884199	31.929050
595.684741	46760.964334	31.934068
596.472418	46825.965500	31.939085
597.322411	46894.489937	31.944103
597.925571	46979.828550	31.949120
598.160113	47052.380107	31.954138
598.786521	47120.263406	31.959156
599.373510	47193.464602	31.964173
599.931913	47277.817302	31.969191
600.674307	47352.730157	31.974208
600.706961	47437.201979	31.979226
601.916772	47509.174244	31.984244
602.054216	47583.385876	31.989261
603.118747	47665.370540	31.994279
603.314340	47741.578337	31.999296
604.218765	47833.151771	32.004314
604.829082	47908.969657	32.009332
605.244348	47986.016854	32.014349
606.025105	48072.458397	32.019367
606.560269	48163.093399	32.024384
607.450695	48230.296050	32.029402
608.090512	48307.847456	32.034420
608.464133	48400.635487	32.039437
609.212690	48478.276997	32.044455
610.016036	48563.813906	32.049472
610.408265	48647.461216	32.054490
611.149171	48715.583963	32.059508
611.497637	48797.846534	32.064525
612.188163	48873.171869	32.069543
613.032882	48965.824855	32.074560
613.619857	49050.496524	32.079578
614.043342	49133.054475	32.084596
614.759985	49220.841338	32.089613
614.969002	49292.101441	32.094631
616.163568	49372.616184	32.099648
616.073887	49465.125915	32.104666
617.150618	49539.657444	32.109684
617.708490	49625.877593	32.114701
618.379563	49717.116532	32.119719
619.013148	49802.421770	32.124736
619.404009	49888.500152	32.129754
620.227108	49979.080459	32.134772
620.429749	50062.894776	32.139789
620.981035	50161.352957	32.144807
622.326014	50250.758805	32.149824
622.470140	50341.449809	32.154842
622.913995	50434.318250	32.159860
623.423828	50526.134042	32.164877
624.067351	50614.021497	32.169895
624.955030	50707.787530	32.174912
625.327249	50815.734354	32.179930
626.565303	50886.982039	32.184948
626.608238	50983.428166	32.189965
627.430287	51078.381723	32.194983
628.000950	51166.729060	32.200000
628.614435	51262.864435	32.205018
629.052501	51354.768683	32.210036
629.675859	51439.953406	32.215053
630.657170	51531.958280	32.220071
631.497426	51626.409358	32.225088
632.004920	51719.895699	32.230106
632.284888	51791.737673	32.235124
632.984138	51880.240758	32.240141
633.789379	51972.703201	32.245159
634.496989	52056.875516	32.250176
635.058932	52128.062593	32.255194
635.755840	52223.497281	32.260212
636.295501	52303.642939	32.265229
636.964358	52375.318627	32.270247
637.912586	52470.940441	32.275264
638.552468	52563.638326	32.280282
638.995525	52634.581587	32.285300
639.392865	52727.895168	32.290317
640.014517	52816.851238	32.295335
640.652807	52903.012786	32.300352
641.084646	53001.047215	32.305370
642.041150	53079.045726	32.310388
642.372213	53162.182683	32.315405
642.943269	53270.031420	32.320423
643.878783	53354.080135	32.325440
644.329547	53463.314348	32.330458
645.310937	53560.464855	32.335476
645.844751	53660.248313	32.340493
646.459988	53742.317399	32.345511
647.447915	53832.146288	32.350528
647.848719	53924.410027	32.355546
648.711996	54005.738018	32.360564
649.391979	54104.021311	32.365581
649.898122	54208.935677	32.370599
650.698669	54291.999921	32.375616
650.941118	54394.172769	32.380634
651.687188	54493.192588	32.385652
652.355830	54579.546074	32.390669
652.937270	54682.927984	32.395687
653.482386	54782.279389	32.400704
654.173590	54877.203669	32.405722
654.861718	54987.677086	32.410740
655.839424	55084.911607	32.415757
656.253787	55182.441820	32.420775
656.880539	55275.786567	32.425792
657.589816	55380.970608	32.430810
658.299935	55473.999267	32.435828
659.149000	55568.306931	32.440845
659.831170	55678.399823	32.445863
660.368011	55766.795765	32.450880
660.847066	55862.543289	32.455898
661.865251	55964.621473	32.460916
662.697589	56061.891158	32.465933
663.383542	56161.794918	32.470951
664.409560	56250.750384	32.475968
664.733383	56342.697030	32.480986
665.229358	56431.241705	32.486004
665.950982	56517.620236	32.491021
666.668725	56620.610729	32.496039
667.601179	56708.395861	32.501056
668.091901	56806.035235	32.506074
668.694115	56906.215647	32.511092
669.330248	56994.392184	32.516109
669.730749	57100.817952	32.521127
670.447452	57204.291862	32.526144
671.022610	57298.412931	32.531162
671.536201	57391.678966	32.536180
672.093202	57496.665647	32.541197
672.492968	57594.292333	32.546215
673.546961	57689.947439	32.551232
674.628598	57808.731301	32.556250
674.860106	57913.622291	32.561268
675.928807	58011.513360	32.566285
676.404147	58114.570604	32.571303
677.285039	58191.072759	32.576320
677.297007	58292.861534	32.581338
678.023419	58385.364093	32.586356
678.788135	58479.396260	32.591373
678.926706	58583.415152	32.596391
680.106241	58685.859853	32.601408
680.166718	58790.044375	32.606426
680.659284	58903.049021	32.611444
681.921042	59011.105792	32.616461
682.223905	59121.583762	32.621479
682.839137	59228.870121	32.626496
683.454670	59358.918826	32.631514
684.686699	59456.815292	32.636532
685.376844	59572.780094	32.641549
685.784482	59680.633976	32.646567
686.490964	59787.706039	32.651584
686.849508	59904.782855	32.656602
687.766214	60014.058471	32.661620
688.306027	60126.449225	32.666637
689.543336	60252.432413	32.671655
690.327819	60360.638476	32.676672
690.743473	60466.138060	32.681690
691.439864	60570.441667	32.686708
692.158722	60696.753400	32.691725
692.807489	60814.299466	32.696743
693.791459	60936.524325	32.701760
694.236712	61047.791964	32.706778
695.344743	61154.356276	32.711796
696.176157	61270.604557	32.716813
696.585038	61379.826087	32.721831
697.429159	61482.757560	32.726848
697.791642	61607.522268	32.731866
698.693291	61710.729795	32.736884
700.057923	61819.593620	32.741901
700.586270	61935.017286	32.746919
701.448055	62041.323573	32.751936
702.060884	62145.649101	32.756954
702.576344	62258.833102	32.761972
703.309331	62362.059156	32.766989
704.062271	62473.012034	32.772007
705.307011	62585.691886	32.777024
706.090612	62676.144315	32.782042
706.565081	62783.238953	32.787060
707.030796	62897.515489	32.792077
708.125604	63003.598713	32.797095
708.287511	63102.264723	32.802112
709.116170	63224.080258	32.807130
709.727121	63327.938117	32.812148
710.394665	63436.211502	32.817165
711.081598	63546.340493	32.822183
711.655401	63645.642681	32.827200
712.643963	63775.993132	32.832218
713.085395	63889.299526	32.837236
713.911982	63999.881940	32.842253
714.244340	64118.472728	32.847271
715.178754	64227.439423	32.852288
716.043594	64343.339431	32.857306
716.660497	64466.088548	32.862324
717.732083	64571.911939	32.867341
717.929417	64696.033809	32.872359
718.802365	64792.947097	32.877376
719.615508	64909.054777	32.882394
720.438156	65032.708795	32.887412
721.550590	65132.573957	32.892429
722.222601	65239.288495	32.897447
722.879424	65355.885942	32.902464
723.502484	65453.336645	32.907482
724.066266	65563.572627	32.912500
725.212626	65657.720413	32.917517
725.875164	65758.472009	32.922535
726.395178	65861.845659	32.927552
727.062259	65966.453471	32.932570
727.502935	66063.197576	32.937588
728.822263	66154.929609	32.942605
729.086691	66271.597013	32.947623
729.796073	66373.152995	32.952640
730.696698	66480.449351	32.957658
731.042197	66596.492012	32.962676
732.057686	66694.250387	32.967693
732.528077	66809.900646	32.972711
733.112639	66923.301182	32.977728
733.978831	67035.069106	32.982746
734.609003	67148.084037	32.987764
735.458024	67255.772211	32.992781
736.129837	67367.207359	32.997799
736.431137	67493.541387	33.002816
737.643644	67611.576943	33.007834
737.993765	67741.147471	33.012852
738.856113	67852.376731	33.017869
739.752771	67985.948751	33.022887
740.244081	68103.739512	33.027904
740.692767	68230.376063	33.032922
741.454622	68359.667474	33.037940
742.271005	68490.758778	33.042957
743.093413	68624.581041	33.047975
743.610162	68737.964674	33.052992
744.712793	68876.167737	33.058010
745.174429	69012.037196	33.063028
745.915316	69127.965369	33.068045
746.984198	69273.440848	33.073063
747.907552	69396.914445	33.078080
749.241688	69512.449616	33.083098
749.372525	69641.941618	33.088116
750.414476	69762.426251	33.093133
750.932655	69884.414292	33.098151
751.624564	70015.168928	33.103168
752.704610	70138.507176	33.108186
753.445169	70268.926573	33.113204
754.244992	70386.767653	33.118221
754.878781	70517.345306	33.123239
756.036091	70638.985562	33.128256
756.878528	70753.312556	33.133274
757.337783	70883.883346	33.138292
758.367192	70998.945838	33.143309
758.951674	71129.769335	33.148327
759.470691	71265.915648	33.153344
760.254990	71390.188879	33.158362
760.739821	71522.232590	33.163380
761.760762	71648.238667	33.168397
762.424937	71774.158974	33.173415
762.999860	71907.638157	33.178432
763.768405	72040.751076	33.183450
764.223147	72174.511016	33.188468
765.173196	72302.878537	33.193485
766.224896	72444.002918	33.198503
766.834194	72576.367705	33.203520
767.890781	72697.290179	33.208538
768.346476	72835.233769	33.213556
769.428566	72966.713501	33.218573
770.125911	73094.975726	33.223591
770.722325	73226.701656	33.228608
771.815920	73358.238790	33.233626
772.573685	73491.254975	33.238644
773.145762	73606.843316	33.243661
774.177072	73744.666054	33.248679
774.669162	73878.443061	33.253696
775.662872	73977.288355	33.258714
776.179627	74112.472911	33.263732
777.122755	74231.898717	33.268749
777.649053	74348.788623	33.273767
778.680602	74472.197774	33.278784
779.355746	74601.484412	33.283802
779.994024	74727.514788	33.288820
780.724282	74853.891168	33.293837
781.393210	74982.036469	33.298855
781.863640	75120.795336	33.303872
782.590481	75253.005318	33.308890
783.164086	75383.002687	33.313908
783.983847	75519.107212	33.318925
785.368326	75660.349403	33.323943
785.550036	75798.711243	33.328960
786.894348	75936.666953	33.333978
787.234621	76086.489227	33.338996
787.812420	76217.850587	33.344013
788.650709	76372.228295	33.349031
789.465981	76522.234409	33.354048
790.216028	76658.755971	33.359066
790.798556	76807.967644	33.364084
791.751941	76958.301775	33.369101
792.737955	77125.859665	33.374119
793.384398	77275.342234	33.379136
794.348650	77411.801474	33.384154
795.124927	77571.750887	33.389172
795.418157	77727.031341	33.394189
796.704215	77870.068605	33.399207
797.550191	78025.538172	33.404224
798.304264	78170.606948	33.409242
798.979069	78338.364574	33.414260
799.983128	78477.056511	33.419277
800.800932	78628.132790	33.424295
801.373819	78789.617284	33.429312
802.609753	78935.452722	33.434330
803.324951	79101.489018	33.439348
804.355534	79253.236498	33.444365
805.251099	79391.806580	33.449383
805.735624	79549.237735	33.454400
806.286231	79699.644326	33.459418
807.236125	79851.099257	33.464436
807.989474	80000.228299	33.469453
809.178027	80162.974704	33.474471
809.896367	80314.047200	33.479488
810.935475	80462.404704	33.484506
811.803239	80616.237789	33.489524
812.636145	80765.687716	33.494541
813.707268	80922.133419	33.499559
814.172955	81076.105628	33.504576
815.001283	81217.449779	33.509594
815.771445	81374.340516	33.514612
816.457218	81526.413355	33.519629
817.337914	81674.646865	33.524647
817.802911	81825.037537	33.529664
818.632267	81984.086193	33.534682
819.642222	82144.820487	33.539700
820.643295	82303.317974	33.544717
821.491357	82461.133314	33.549735
822.132211	82608.394043	33.554752
823.076513	82754.859132	33.559770
824.308488	82916.264436	33.564788
824.786332	83061.170035	33.569805
825.837982	83228.187075	33.574823
826.608517	83389.089907	33.579840
827.482798	83522.779654	33.584858
828.283211	83676.087930	33.589876
829.045394	83826.107464	33.594893
830.001360	83967.789294	33.599911
830.625373	84115.144778	33.604928
831.622478	84247.236846	33.609946
832.334106	84381.249490	33.614964
833.207028	84531.634955	33.619981
834.253594	84679.683490	33.624999
835.118809	84808.909272	33.630016
835.550187	84949.911929	33.635034
836.175311	85103.315630	33.640052
837.228263	85242.041018	33.645069
838.375113	85390.286351	33.650087
838.711517	85544.904811	33.655104
839.566210	85703.576562	33.660122
840.451790	85855.525014	33.665140
841.345310	85999.779454	33.670157
842.505209	86151.380853	33.675175
843.189120	86305.674948	33.680192
843.698081	86456.107741	33.685210
844.313890	86615.666697	33.690228
844.890449	86775.397738	33.695245
846.141737	86943.724839	33.700263
846.909340	87108.279665	33.705280
847.753254	87264.926460	33.710298
848.418473	87441.010075	33.715316
849.335675	87604.436395	33.720333
850.331970	87761.592868	33.725351
851.065022	87944.072533	33.730368
852.078295	88123.767485	33.735386
852.701644	88278.774339	33.740404
853.524122	88448.638447	33.745421
854.593989	88617.627669	33.750439
855.309097	88792.226171	33.755456
856.107552	88963.249623	33.760474
856.772239	89141.484899	33.765492
857.695869	89311.363839	33.770509
858.938134	89485.355209	33.775527
859.750023	89674.846691	33.780544
860.698118	89834.695404	33.785562
861.668639	90004.255174	33.790580
862.247635	90175.475505	33.795597
863.319005	90359.999968	33.800615
864.427065	90534.951454	33.805632
865.289199	90688.036197	33.810650
866.191386	90864.840328	33.815668
866.646852	91034.024187	33.820685
867.979044	91198.197905	33.825703
868.828342	91372.767932	33.830720
869.680947	91547.705743	33.835738
870.810838	91719.149967	33.840756
871.322218	91886.197887	33.845773
872.654620	92047.232067	33.850791
873.364608	92219.071961	33.855808
874.250885	92393.130686	33.860826
874.890334	92560.446942	33.865844
875.586751	92728.742254	33.870861
876.834480	92897.574271	33.875879
877.667829	93071.703597	33.880896
878.458238	93247.258962	33.885914
879.162371	93413.589458	33.890932
879.825349	93593.706293	33.895949
880.664677	93767.542171	33.900967
881.670413	93955.776002	33.905984
882.849824	94128.564634	33.911002
883.659184	94300.459876	33.916020
884.794520	94489.714442	33.921037
885.612727	94641.489754	33.926055
886.295292	94831.176173	33.931072
886.952389	94999.094971	33.936090
888.024244	95160.243513	33.941108
888.716823	95331.329806	33.946125
889.623954	95500.552621	33.951143
889.984160	95656.118982	33.956160
891.003521	95843.371368	33.961178
891.987506	96010.964619	33.966196
892.890126	96188.497494	33.971213
893.789630	96367.234825	33.976231
894.721807	96555.956551	33.981248
895.633122	96720.021912	33.986266
896.367157	96890.643791	33.991284
897.246338	97077.599541	33.996301
898.318898	97259.682305	34.001319
899.107915	97438.008849	34.006336
899.898495	97625.597378	34.011354
900.902374	97803.707499	34.016372
901.128718	98002.533125	34.021389
902.584695	98185.344312	34.026407
903.246827	98373.656016	34.031424
904.042382	98565.688350	34.036442
905.131030	98759.712157	34.041460
906.204761	98953.739933	34.046477
907.174412	99143.133476	34.051495
907.797407	99330.648537	34.056512
909.134362	99518.483926	34.061530
909.914841	99708.799253	34.066548
910.700106	99909.187364	34.071565
911.897398	100101.988112	34.076583
912.635811	100298.981114	34.081600
913.360939	100500.795617	34.086618
914.869743	100683.768221	34.091636
915.557542	100880.907060	34.096653
917.112401	101070.459030	34.101671
917.853029	101263.337695	34.106688
918.800276	101447.833013	34.111706
919.870856	101624.104167	34.116724
920.744878	101821.029615	34.121741
921.666095	102002.260029	34.126759
922.540273	102197.042069	34.131776
923.207499	102385.642413	34.136794
924.293839	102567.913233	34.141812
925.229989	102770.812539	34.146829
926.324314	102952.312341	34.151847
927.739159	103142.023110	34.156864
928.462246	103322.117910	34.161882
929.750833	103513.530123	34.166900
930.474641	103710.830456	34.171917
931.590178	103884.146517	34.176935
932.883152	104061.334786	34.181952
933.217511	104237.093269	34.186970
934.383080	104398.944022	34.191988
935.445664	104591.756539	34.197005
936.222294	104769.370489	34.202023
937.170683	104949.357099	34.207040
938.074642	105141.984601	34.212058
939.018271	105326.236029	34.217076
939.758352	105512.668940	34.222093
940.624730	105689.292868	34.227111
941.913486	105875.321169	34.232128
942.240482	106063.637207	34.237146
943.542488	106241.079442	34.242164
944.798359	106442.973168	34.247181
945.368865	106616.865982	34.252199
946.404148	106804.259845	34.257216
947.242492	106994.473828	34.262234
948.017183	107180.659569	34.267252
948.780250	107365.138760	34.272269
949.583112	107564.709512	34.277287
950.930051	107741.293200	34.282304
951.554938	107916.072151	34.287322
952.602737	108101.813988	34.292340
953.478628	108278.580347	34.297357
954.062543	108473.115218	34.302375
954.830919	108660.426956	34.307392
955.564529	108852.546070	34.312410
956.493662	109043.063719	34.317428
957.508165	109250.680314	34.322445
958.211220	109444.607288	34.327463
959.644083	109653.766520	34.332480
960.290765	109863.994483	34.337498
961.168919	110055.693036	34.342516
962.059021	110281.184989	34.347533
962.683991	110494.816062	34.352551
964.042349	110695.027784	34.357568
964.805607	110912.717981	34.362586
965.366926	111134.509318	34.367604
966.466501	111344.218020	34.372621
967.277615	111564.489597	34.377639
968.533008	111784.512267	34.382656
969.450135	112012.522250	34.387674
970.649297	112234.761937	34.392692
971.333612	112462.244082	34.397709
972.327842	112687.510798	34.402727
973.546449	112899.175269	34.407744
974.663014	113138.739937	34.412762
975.687743	113362.588368	34.417780
976.503449	113577.111507	34.422797
977.620645	113790.332400	34.427815
979.185135	114030.869652	34.432832
979.964836	114253.296253	34.437850
981.262445	114465.111721	34.442868
981.948092	114691.383210	34.447885
982.363237	114910.264749	34.452903
983.991387	115127.098119	34.457920
984.767409	115357.870147	34.462938
985.914047	115581.044915	34.467956
987.106409	115802.414922	34.472973
987.925604	116037.264837	34.477991
989.324770	116236.572614	34.483008
990.396319	116468.977335	34.488026
991.192730	116690.812465	34.493044
992.153034	116908.263985	34.498061
992.877942	117128.239277	34.503079
993.708419	117365.062182	34.508096
994.192297	117590.642847	34.513114
995.661628	117824.754147	34.518132
996.531402	118058.535581	34.523149
997.590674	118287.891130	34.528167
998.830695	118513.328937	34.533184
999.752975	118758.472600	34.538202
1001.005424	118979.388738	34.543220
1001.858169	119197.471028	34.548237
1002.758900	119438.316100	34.553255
1003.926673	119682.400814	34.558272
1004.881916	119905.894618	34.563290
1006.018200	120140.599352	34.568308
1007.149399	120373.558234	34.573325
1007.788997	120594.081103	34.578343
1008.976552	120828.073367	34.583360
1009.857942	121072.065040	34.588378
1010.772289	121295.170834	34.593396
1011.991136	121523.347354	34.598413
1012.768341	121758.998788	34.603431
1013.841427	121991.524048	34.608448
1014.704456	122236.187413	34.613466
1015.843716	122452.789616	34.618484
1017.025660	122685.201030	34.623501
1017.624658	122913.883544	34.628519
1018.965232	123127.961078	34.633536
1019.444126	123361.811803	34.638554
1020.497029	123596.596077	34.643572
1021.916882	123817.838096	34.648589
1022.638035	124048.650866	34.653607
1024.034785	124279.417256	34.658624
1024.697094	124508.823970	34.663642
1025.815713	124752.173327	34.668660
1026.876333	124981.036342	34.673677
1027.845812	125205.911459	34.678695
1029.121433	125431.016532	34.683712
1029.855380	125674.196095	34.688730
1031.123610	125912.853735	34.693748
1032.227568	126141.426951	34.698765
1033.287071	126382.568748	34.703783
1034.205288	126612.811085	34.708800
1035.322052	126845.607842	34.713818
1036.117528	127090.056016	34.718836
1037.512257	127340.376667	34.723853
1038.503299	127577.711721	34.728871
1039.471737	127812.073921	34.733888
1040.611933	128061.187763	34.738906
1041.747719	128308.010297	34.743924
1042.509196	128542.969929	34.748941
1043.447891	128794.036830	34.753959
1044.641246	129038.967217	34.758976
1045.583681	129290.088239	34.763994
1046.714912	129525.742128	34.769012
1047.551202	129795.199973	34.774029
1048.950287	130040.700048	34.779047
1049.944782	130284.646430	34.784064
1051.230800	130530.574642	34.789082
1052.174430	130772.251684	34.794100
1053.501046	131018.329137	34.799117
1054.754034	131278.642686	34.804135
1056.086087	131517.079777	34.809152
1057.055703	131752.739134	34.814170
1058.237625	132016.454954	34.819188
1059.053948	132242.370169	34.824205
1059.774336	132484.769048	34.829223
1061.070725	132749.549547	34.834240
1062.189654	133007.567063	34.839258
1063.337389	133238.885461	34.844276
1064.292475	133479.465808	34.849293
1064.953495	133741.481884	34.854311
1066.104500	133995.407555	34.859328
1067.584156	134233.713908	34.864346
1068.830757	134486.727634	34.869364
1069.960436	134723.257245	34.874381
1071.121809	134973.575993	34.879399
1072.378344	135216.642315	34.884416
1073.203011	135465.359744	34.889434
1073.857818	135710.696914	34.894452
1075.043454	135954.883397	34.899469
1075.917035	136209.049737	34.904487
1077.068438	136455.692385	34.909504
1078.153969	136723.823850	34.914522
1079.231457	136973.575968	34.919540
1080.339002	137220.256964	34.924557
1081.410004	137493.988078	34.929575
1082.304940	137740.264331	34.934592
1083.150601	137982.151209	34.939610
1084.212923	138245.151522	34.944628
1085.648030	138511.756442	34.949645
1086.716558	138767.469769	34.954663
1088.224831	139006.731693	34.959680
1088.923672	139264.449684	34.964698
1089.837778	139493.315204	34.969716
1091.213938	139743.051531	34.974733
1091.840183	139991.353994	34.979751
1093.042588	140243.519046	34.984768
1093.940943	140482.968250	34.989786
1095.159458	140742.779908	34.994804
1096.367900	140988.571848	34.999821
1097.104364	141237.435830	35.004839
1098.392324	141485.183548	35.009856
1099.502296	141753.630257	35.014874
1100.530848	142001.449902	35.019892
1101.903977	142243.495857	35.024909
1102.527862	142518.977348	35.029927
1103.735048	142761.713702	35.034944
1104.912559	143036.664139	35.039962
1105.859865	143301.447194	35.044980
1106.983777	143550.872628	35.049997
1108.231717	143821.265438	35.055015
1110.006155	144076.230036	35.060032
1111.272601	144337.328997	35.065050
1112.323680	144595.384055	35.070068
1113.749052	144854.862877	35.075085
1114.910619	145113.562909	35.080103
1115.885790	145357.103823	35.085120
1116.847560	145625.376675	35.090138
1117.943409	145885.348640	35.095156
1119.270765	146137.358523	35.100173
1119.930101	146409.035079	35.105191
1121.352518	146664.279426	35.110208
1122.205664	146920.976495	35.115226
1123.191895	147193.682990	35.120244
1124.550999	147450.173516	35.125261
1125.576410	147718.134573	35.130279
1126.845638	147996.672119	35.135296
1128.169576	148258.728880	35.140314
1129.128122	148526.643566	35.145332
1130.416729	148798.589406	35.150349
1131.037038	149069.113044	35.155367
1132.347336	149341.300320	35.160384
1133.306430	149617.022592	35.165402
1134.097812	149907.207373	35.170420
1135.418084	150173.400335	35.175437
1136.525291	150459.669132	35.180455
1137.682100	150743.940754	35.185472
1138.515697	151025.604494	35.190490
1139.354218	151310.414953	35.195508
1140.744617	151606.284970	35.200525
1141.781924	151902.101471	35.205543
1142.735496	152192.239313	35.210560
1144.282305	152481.698034	35.215578
1145.134685	152783.868366	35.220596
1146.694495	153071.655250	35.225613
1147.458523	153357.647757	35.230631
1149.097631	153665.200004	35.235648
1150.418952	153949.215083	35.240666
1151.775004	154238.439678	35.245684
1153.107189	154509.164275	35.250701
1153.982080	154802.049474	35.255719
1155.318709	155079.563413	35.260736
1156.484007	155368.485536	35.265754
1157.869884	155655.090199	35.270772
1159.156585	155935.878444	35.275789
1160.260748	156215.658708	35.280807
1161.853281	156490.096189	35.285824
1162.740107	156771.172103	35.290842
1163.671275	157054.855812	35.295860
1165.232253	157325.930164	35.300877
1165.987868	157587.257615	35.305895
1166.834530	157860.089930	35.310912
1168.222925	158123.523699	35.315930
1169.163566	158393.718319	35.320948
1170.353729	158660.727591	35.325965
1171.388704	158939.955076	35.330983
1172.541475	159212.492421	35.336000
1173.569892	159499.513868	35.341018
1174.155217	159773.912002	35.346036
1175.631049	160053.150567	35.351053
1176.640175	160355.061845	35.356071
1177.613370	160648.545053	35.361088
1178.828506	160931.879558	35.366106
1179.732921	161222.625353	35.371124
1181.114753	161528.086696	35.376141
1182.217238	161835.423272	35.381159
1183.410030	162134.526352	35.386176
1184.655633	162437.314692	35.391194
1185.722732	162749.078854	35.396212
1186.846580	163048.199908	35.401229
1187.739155	163364.120698	35.406247
1189.152635	163684.563277	35.411264
1190.314229	163997.780165	35.416282
1191.561781	164310.325458	35.421300
1192.957705	164614.779452	35.426317
1194.112839	164942.252241	35.431335
1195.091358	165265.379520	35.436352
1196.655604	165572.362770	35.441370
1198.018364	165887.387401	35.446388
1199.547361	166203.249671	35.451405
1200.766004	166516.031583	35.456423
1201.694102	166820.286661	35.461440
1203.355049	167134.205384	35.466458
1204.629337	167468.034435	35.471476
1205.449926	167772.808751	35.476493
1206.757675	168081.514280	35.481511
1207.826293	168397.037055	35.486528
1209.407882	168704.712056	35.491546
1210.643954	169016.366998	35.496564
1212.039489	169334.240631	35.501581
1213.267464	169646.713399	35.506599
1214.511588	169947.829164	35.511616
1215.809860	170257.452285	35.516634
1216.884361	170578.712235	35.521652
1218.187160	170901.193008	35.526669
1219.604203	171208.125633	35.531687
1220.679619	171511.500270	35.536704
1222.037699	171835.590075	35.541722
1223.312117	172147.564856	35.546740
1224.099674	172458.873429	35.551757
1225.811897	172781.147595	35.556775
1226.784892	173082.163841	35.561792
1228.260537	173407.450798	35.566810
1229.221058	173731.010392	35.571828
1230.583812	174036.181501	35.576845
1231.818360	174349.078618	35.581863
1232.856074	174678.799359	35.586880
1234.298400	174984.293410	35.591898
1235.078323	175306.231189	35.596916
1236.304518	175617.386783	35.601933
1237.523718	175952.416351	35.606951
1238.273417	176285.190680	35.611968
1239.420960	176608.104447	35.616986
1240.708146	176947.025726	35.622004
1242.318876	177279.778981	35.627021
1243.747328	177608.135458	35.632039
1244.844911	177935.152735	35.637056
1246.032657	178262.360359	35.642074
1246.817438	178584.966309	35.647092
1248.184318	178907.820940	35.652109
1249.245992	179218.074781	35.657127
1250.593797	179543.474937	35.662144
1251.881916	179859.254210	35.667162
1253.300435	180181.562789	35.672180
1254.434465	180501.128213	35.677197
1256.005662	180835.612428	35.682215
1256.986698	181153.278050	35.687232
1258.307630	181470.940309	35.692250
1259.502736	181809.681282	35.697268
1260.922627	182135.619164	35.702285
1262.244817	182458.986023	35.707303
1262.916253	182793.339526	35.712320
1264.285156	183126.196586	35.717338
1265.350971	183474.692020	35.722356
1266.707373	183804.991571	35.727373
1268.270895	184138.584441	35.732391
1269.345132	184502.697067	35.737408
1270.771082	184839.261711	35.742426
1272.241942	185189.046935	35.747444
1273.114331	185537.118123	35.752461
1274.163857	185884.933833	35.757479
1275.685982	186227.418845	35.762496
1277.146107	186582.139699	35.767514
1278.343129	186936.525470	35.772532
1279.569528	187284.549333	35.777549
1281.181751	187622.813977	35.782567
1282.475263	187991.508654	35.787584
1284.263897	188317.816559	35.792602
1285.143500	188676.505400	35.797620
1286.390842	189036.976401	35.802637
1288.019538	189375.198073	35.807655
1289.158745	189735.158196	35.812672
1290.863086	190080.937069	35.817690
1292.590113	190421.306635	35.822708
1293.427727	190766.712203	35.827725
1295.145036	191113.980297	35.832743
1296.080999	191455.870124	35.837760
1297.697005	191801.077151	35.842778
1298.599729	192161.611746	35.847796
1300.052140	192518.274862	35.852813
1301.599011	192854.130925	35.857831
1302.632980	193212.733324	35.862848
1304.204658	193569.801915	35.867866
1305.733376	193920.494251	35.872884
1306.414813	194262.822929	35.877901
1308.011223	194617.049928	35.882919
1309.014832	194971.414885	35.887936
1310.162308	195316.478069	35.892954
1311.758612	195694.082747	35.897972
1312.736831	196050.070293	35.902989
1313.885958	196404.698642	35.908007
1315.291698	196778.596171	35.913024
1316.792663	197132.345312	35.918042
1317.973807	197490.808415	35.923060
1318.986687	197864.650155	35.928077
1320.667723	198227.617916	35.933095
1321.701023	198588.358598	35.938112
1323.251999	198960.899024	35.943130
1324.681344	199331.417600	35.948148
1325.647633	199692.492764	35.953165
1326.963003	200058.565247	35.958183
1328.459974	200435.490228	35.963200
1329.683953	200796.541482	35.968218
1330.797107	201170.575704	35.973236
1332.204421	201545.299798	35.978253
1334.012345	201903.175330	35.983271
1334.607241	202281.173472	35.988288
1335.903900	202633.207942	35.993306
1337.768976	202985.683616	35.998324
1338.968428	203344.758834	36.003341
1340.683433	203701.338424	36.008359
1341.690324	204057.884297	36.013376
1342.907014	204411.438972	36.018394
1344.437407	204763.965946	36.023412
1345.597828	205123.945251	36.028429
1346.934431	205482.754521	36.033447
1348.246246	205860.691272	36.038464
1349.812633	206220.964436	36.043482
1350.889596	206594.144179	36.048500
1352.584289	206967.617432	36.053517
1353.690433	207320.137655	36.058535
1354.533200	207694.720060	36.063552
1356.196589	208071.835298	36.068570
1357.946552	208447.338209	36.073588
1359.174290	208833.391828	36.078605
1360.678745	209212.354543	36.083623
1361.876336	209584.424130	36.088640
1363.072754	209966.107767	36.093658
1364.588431	210358.851025	36.098676
1366.020561	210732.588709	36.103693
1367.159960	211112.052345	36.108711
1368.496310	211499.281731	36.113728
1370.076265	211876.707999	36.118746
1371.888110	212260.243537	36.123764
1373.036518	212651.788507	36.128781
1374.767719	213013.754065	36.133799
1376.286763	213415.831608	36.138816
1377.581469	213797.224527	36.143834
1378.974015	214179.644231	36.148852
1379.997071	214573.402711	36.153869
1381.477151	214948.243092	36.158887
1383.248134	215342.897422	36.163904
1384.491400	215737.437398	36.168922
1385.942042	216120.084405	36.173940
1387.143220	216517.555372	36.178957
1388.589756	216904.015905	36.183975
1389.845809	217296.833441	36.188992
1391.214887	217688.592666	36.194010
1392.561732	218095.722762	36.199028
1393.928347	218495.841541	36.204045
1395.206216	218948.093073	36.209063
1396.177664	219356.153951	36.214080
1397.739957	219765.185729	36.219098
1399.205457	220169.257112	36.224116
1400.760907	220582.357067	36.229133
1402.116288	220996.253670	36.234151
1403.146519	221403.805174	36.239168
1404.727892	221813.934176	36.244186
1406.277585	222236.058198	36.249204
1407.510419	222641.320586	36.254221
1409.445480	223049.541885	36.259239
1410.612667	223470.946526	36.264256
1411.722082	223862.391393	36.269274
1413.176291	224286.545685	36.274292
1414.607011	224701.714114	36.279309
1416.016872	225125.066103	36.284327
1417.426235	225547.022766	36.289344
1418.912251	225960.688058	36.294362
1420.044576	226388.357579	36.299380
1421.264612	226808.470440	36.304397
1423.064277	227220.640569	36.309415
1424.386257	227652.525052	36.314432
1425.700581	228063.533510	36.319450
1427.424285	228488.826806	36.324468
1428.842619	228900.862237	36.329485
1430.068228	229296.090434	36.334503
1431.467918	229699.876413	36.339520
1432.874231	230106.100976	36.344538
1434.974414	230507.132176	36.349556
1435.761866	230919.100229	36.354573
1437.405627	231322.825411	36.359591
1438.921020	231724.185284	36.364608
1440.455459	232121.631439	36.369626
1441.781658	232540.017956	36.374644
1443.280814	232948.597787	36.379661
1445.009841	233351.349396	36.384679
1446.315117	233763.214795	36.389696
1447.597898	234176.177273	36.394714
1449.368466	234583.573708	36.399732
1450.340741	235000.882422	36.404749
1451.960654	235419.533234	36.409767
1453.387309	235841.112782	36.414784
1454.708984	236263.802999	36.419802
1456.429340	236687.038131	36.424820
1458.004947	237112.228724	36.429837
1459.082337	237533.285905	36.434855
1460.884988	237961.235280	36.439872
1462.041026	238389.749610	36.444890
1463.882800	238818.304196	36.449908
1465.155583	239259.781608	36.454925
1466.876766	239689.170935	36.459943
1468.357672	240101.098892	36.464960
1469.737761	240543.298173	36.469978
1470.909644	240976.032393	36.474996
1472.470691	241407.458594	36.480013
1473.642166	241849.822103	36.485031
1475.280115	242298.333093	36.490048
1476.359716	242743.329999	36.495066
1478.143761	243190.192915	36.500084
1479.485140	243645.461723	36.505101
1481.275406	244090.064503	36.510119
1482.834870	244547.534434	36.515136
1483.846593	244994.147084	36.520154
1485.357898	245454.725692	36.525172
1486.943535	245907.240194	36.530189
1488.292707	246353.723221	36.535207
1489.879478	246826.281726	36.540224
1491.225490	247290.497812	36.545242
1492.624842	247744.976537	36.550260
1494.000111	248223.414754	36.555277
1495.559691	248684.650924	36.560295
1497.294516	249148.703928	36.565312
1498.540183	249631.585619	36.570330
1500.413854	250108.115186	36.575348
1501.639442	250577.868075	36.580365
1503.148767	251041.503370	36.585383
1504.698683	251514.150558	36.590400
1506.488779	251985.691688	36.595418
1508.104116	252444.509777	36.600436
1509.810101	252915.532235	36.605453
1511.415896	253382.430937	36.610471
1513.357272	253843.076285	36.615488
1514.431600	254312.578353	36.620506
1516.190475	254765.303312	36.625524
1517.774058	255228.167974	36.630541
1519.349422	255702.770573	36.635559
1520.900102	256157.613797	36.640576
1522.476687	256626.399367	36.645594
1524.131358	257087.881534	36.650612
1525.227253	257552.885535	36.655629
1526.765619	258007.096507	36.660647
1528.244225	258471.326373	36.665664
1529.545771	258923.874655	36.670682
1531.704801	259346.178621	36.675700
1532.815622	259804.550481	36.680717
1534.316798	260245.939374	36.685735
1536.080459	260691.476524	36.690752
1537.468920	261141.648181	36.695770
1539.072014	261581.750096	36.700788
1540.320588	262029.226620	36.705805
1541.264633	262479.166641	36.710823
1543.196798	262932.627009	36.715840
1544.510783	263404.682860	36.720858
1546.449294	263848.006022	36.725876
1547.776597	264317.646058	36.730893
1549.237299	264787.416309	36.735911
1550.953375	265257.728477	36.740928
1552.537287	265723.159384	36.745946
1553.935046	266187.325178	36.750964
1555.784586	266669.503215	36.755981
1557.317430	267126.406200	36.760999
1558.759763	267614.061617	36.766016
1559.998229	268105.154293	36.771034
1562.027396	268560.348477	36.776052
1563.678319	269034.656996	36.781069
1565.484476	269519.888166	36.786087
1567.173323	269980.954490	36.791104
1568.444334	270475.799074	36.796122
1569.816330	270947.865340	36.801140
1571.405850	271425.483805	36.806157
1572.899951	271917.368456	36.811175
1574.078046	272405.113108	36.816192
1575.832940	272903.405702	36.821210
1577.205370	273396.578489	36.826228
1578.966781	273907.290459	36.831245
1580.559393	274405.963144	36.836263
1582.372547	274901.702702	36.841280
1583.728160	275397.567706	36.846298
1584.976188	275897.996642	36.851316
1586.753230	276426.254757	36.856333
1588.196961	276921.772179	36.861351
1590.394599	277424.200711	36.866368
1591.745790	277934.464797	36.871386
1593.613643	278444.490124	36.876404
1595.512154	278946.964789	36.881421
1596.941221	279459.778280	36.886439
1598.349987	279956.869979	36.891456
1599.925970	280477.404463	36.896474
1601.458627	280983.948266	36.901492
1603.065325	281499.267660	36.906509
1604.980131	281998.861896	36.911527
1606.940228	282510.894258	36.916544
1608.502496	283015.395734	36.921562
1610.468779	283520.006974	36.926580
1612.500836	284011.701916	36.931597
1613.911228	284506.393827	36.936615
1615.863274	285003.763706	36.941632
1617.234749	285502.548777	36.946650
1618.864069	286003.093291	36.951668
1620.705858	286488.995483	36.956685
1622.555296	286968.443029	36.961703
1624.423293	287467.470273	36.966720
1626.077132	287972.703664	36.971738
1627.290653	288442.040303	36.976756
1629.371331	288936.734814	36.981773
1630.741869	289439.190426	36.986791
1632.142992	289922.461721	36.991808
1633.173318	290412.879284	36.996826
1634.908919	290910.417872	37.001844
1636.544337	291397.150597	37.006861
1637.811204	291886.660181	37.011879
1639.795037	292361.850937	37.016896
1641.080968	292843.581315	37.021914
1642.447203	293340.511221	37.026932
1644.103306	293825.935976	37.031949
1645.388405	294310.073842	37.036967
1646.987924	294811.226504	37.041984
1648.544383	295312.663570	37.047002
1649.618771	295813.797050	37.052020
1651.376375	296335.312943	37.057037
1652.787517	296844.996776	37.062055
1654.450325	297360.224601	37.067072
1656.021620	297885.345361	37.072090
1657.507525	298413.754158	37.077108
1659.424798	298946.280006	37.082125
1660.789268	299482.831193	37.087143
1662.382429	300012.001749	37.092160
1663.925505	300573.586204	37.097178
1665.854749	301113.820149	37.102196
1667.640122	301667.764520	37.107213
1669.178373	302215.930454	37.112231
1670.921734	302761.189543	37.117248
1672.574132	303308.263814	37.122266
1674.338247	303867.227972	37.127284
1676.346175	304417.919856	37.132301
1677.624569	304976.627391	37.137319
1679.762967	305529.195952	37.142336
1681.258335	306082.476776	37.147354
1682.726292	306638.882525	37.152372
1684.783603	307199.555775	37.157389
1686.348242	307767.087575	37.162407
1688.198333	308331.368643	37.167424
1689.551431	308901.518302	37.172442
1691.208016	309473.747315	37.177460
1693.290267	310034.550293	37.182477
1694.799709	310611.138441	37.187495
1696.951760	311182.512036	37.192512
1698.562074	311753.742414	37.197530
1700.412830	312311.825209	37.202548
1702.345638	312889.393780	37.207565
1704.411223	313441.185993	37.212583
1706.062882	314014.043801	37.217600
1707.407487	314586.871801	37.222618
1709.204815	315154.135658	37.227636
1711.299252	315713.372523	37.232653
1712.652363	316284.078467	37.237671
1714.383344	316857.104630	37.242688
1715.809362	317434.341094	37.247706
1717.711678	318013.170297	37.252724
1719.650074	318589.805058	37.257741
1721.373621	319164.870810	37.262759
1722.793273	319731.246949	37.267776
1724.781533	320324.288100	37.272794
1726.760956	320900.922311	37.277812
1728.427549	321462.850571	37.282829
1729.803408	322045.490878	37.287847
1731.752455	322620.794976	37.292864
1733.517598	323213.491959	37.297882
1734.569692	323801.019881	37.302900
1736.706277	324379.299076	37.307917
1738.023643	324969.844854	37.312935
1739.836210	325558.856205	37.317952
1741.483207	326157.918410	37.322970
1743.097808	326736.414502	37.327988
1744.939448	327343.557884	37.333005
1746.719463	327945.043609	37.338023
1748.633728	328532.714994	37.343040
1750.506751	329120.565166	37.348058
1752.192482	329698.843584	37.353076
1754.119358	330250.038054	37.358093
1755.541207	330833.604243	37.363111
1757.573648	331390.635176	37.368128
1759.816696	331951.357959	37.373146
1761.525579	332527.395743	37.378164
1763.620276	333075.692180	37.383181
1765.222037	333650.416084	37.388199
1766.917231	334207.601973	37.393216
1768.586356	334777.835112	37.398234
1770.769589	335335.182994	37.403252
1772.499377	335890.696066	37.408269
1774.140190	336474.269083	37.413287
1775.887690	337029.742146	37.418304
1777.253445	337603.346488	37.423322
1778.875168	338191.955507	37.428340
1780.994556	338753.898410	37.433357
1782.697210	339350.857921	37.438375
1784.541034	339919.890476	37.443392
1786.366974	340503.159853	37.448410
1787.909183	341098.171049	37.453428
1790.042683	341684.955191	37.458445
1791.412219	342275.209032	37.463463
1793.119557	342866.821594	37.468480
1794.764815	343469.960788	37.473498
1796.642549	344076.582310	37.478516
1798.479259	344675.207939	37.483533
1799.677696	345293.221103	37.488551
1802.226312	345895.242173	37.493568
1804.107639	346494.853086	37.498586
1805.960012	347100.476300	37.503604
1808.189617	347721.688842	37.508621
1810.087602	348315.588809	37.513639
1811.757719	348935.354735	37.518656
1813.605689	349537.495520	37.523674
1815.459260	350147.241018	37.528692
1817.269421	350760.741482	37.533709
1818.749903	351376.521261	37.538727
1820.548434	351991.910239	37.543744
1822.251546	352609.768054	37.548762
1823.728199	353263.181991	37.553780
1825.611301	353878.860739	37.558797
1827.264481	354517.356367	37.563815
1828.811789	355162.330852	37.568832
1830.871784	355798.405936	37.573850
1832.378837	356442.784236	37.578868
1834.388617	357076.514092	37.583885
1836.472762	357724.812269	37.588903
1838.533352	358359.326429	37.593920
1841.002704	359004.826265	37.598938
1842.782121	359632.364365	37.603956
1844.490918	360275.711623	37.608973
1846.712277	360913.458477	37.613991
1848.523405	361540.099451	37.619008
1850.129340	362185.513950	37.624026
1851.836364	362835.899467	37.629044
1853.549290	363463.465353	37.634061
1855.536979	364113.225540	37.639079
1857.507218	364755.189409	37.644096
1859.549992	365392.894127	37.649114
1861.558859	366042.694916	37.654132
1863.483919	366664.999271	37.659149
1865.511236	367309.448306	37.664167
1866.892663	367959.244097	37.669184
1869.573908	368582.077424	37.674202
1871.252562	369209.302092	37.679220
1873.507142	369848.926859	37.684237
1875.402717	370466.480863	37.689255
1877.094747	371071.299351	37.694272
1878.986689	371678.104155	37.699290
1880.924748	372273.933810	37.704308
1882.831761	372856.011465	37.709325
1884.640019	373473.757558	37.714343
1886.307922	374066.710884	37.719360
1888.180321	374668.599170	37.724378
1889.465631	375280.389442	37.729396
1891.541147	375885.520794	37.734413
1893.125686	376500.233380	37.739431
1894.771916	377140.844154	37.744448
1896.264289	377751.441504	37.749466
1898.499518	378409.430707	37.754484
1900.113605	379051.127448	37.759501
1901.991577	379691.323214	37.764519
1903.935710	380338.317607	37.769536
1905.750699	380987.527173	37.774554
1907.394761	381646.008086	37.779572
1909.242003	382301.704012	37.784589
1910.943870	382966.564888	37.789607
1912.777274	383644.398578	37.794624
1914.520238	384316.629679	37.799642
1916.347631	384988.402089	37.804660
1918.305348	385678.749603	37.809677
1920.179188	386373.482592	37.814695
1921.748739	387064.701355	37.819712
1924.041168	387757.763591	37.824730
1925.782458	388465.504801	37.829748
1927.971148	389158.401633	37.834765
1929.680327	389861.857888	37.839783
1931.602854	390586.557958	37.844800
1933.873580	391280.814210	37.849818
1935.824986	391992.446854	37.854836
1937.842266	392700.604807	37.859853
1939.568575	393425.296368	37.864871
1942.067320	394136.687816	37.869888
1944.170390	394838.749402	37.874906
1946.240475	395562.268865	37.879924
1948.164025	396266.684149	37.884941
1950.038658	396974.309843	37.889959
1951.816207	397700.816745	37.894976
1954.400735	398412.473062	37.899994
1956.249982	399130.214609	37.905012
1958.091909	399832.936717	37.910029
1960.176846	400541.329243	37.915047
1962.188945	401266.416797	37.920064
1964.267818	401968.845450	37.925082
1966.440037	402695.543188	37.930100
1968.366028	403412.481867	37.935117
1970.627482	404120.250354	37.940135
1972.394145	404836.748596	37.945152
1974.433399	405552.398191	37.950170
1976.605211	406266.740796	37.955188
1978.373491	406984.070733	37.960205
1980.650481	407700.462151	37.965223
1981.814354	408413.522298	37.970240
1984.214451	409137.330020	37.975258
1986.152624	409871.277743	37.980276
1988.017177	410580.289760	37.985293
1990.227317	411297.231376	37.990311
1992.140709	412017.521374	37.995328
1994.453667	412728.480184	38.000346
1996.316920	413454.591339	38.005364
1998.606930	414177.344704	38.010381
2000.628715	414893.714242	38.015399
2002.709010	415607.800392	38.020416
2004.400293	416314.636794	38.025434
2006.010305	417036.689131	38.030452
2008.071912	417736.916728	38.035469
2009.969975	418432.973558	38.040487
2011.953384	419126.135736	38.045504
2013.859299	419828.231489	38.050522
2015.940191	420530.203083	38.055540
2017.920024	421225.537282	38.060557
2019.791487	421935.962377	38.065575
2021.404718	422654.588907	38.070592
2023.817064	423365.416104	38.075610
2025.449926	424072.553561	38.080628
2027.256704	424809.772394	38.085645
2029.424252	425528.578981	38.090663
2031.000261	426267.463340	38.095680
2032.991903	427010.206352	38.100698
2034.931678	427751.872005	38.105716
2036.572522	428498.678064	38.110733
2038.600404	429259.826689	38.115751
2040.307490	430030.724732	38.120768
2042.284308	430798.667765	38.125786
2044.140261	431574.199711	38.130804
2045.922767	432365.512840	38.135821
2048.292732	433140.301223	38.140839
2050.208615	433938.980857	38.145856
2052.310895	434720.139269	38.150874
2054.758208	435514.020505	38.155892
2056.460548	436316.703115	38.160909
2058.954267	437125.857564	38.165927
2060.714591	437932.219625	38.170944
2062.871196	438729.327620	38.175962
2065.081277	439543.048718	38.180980
2067.207996	440358.171284	38.185997
2069.528968	441159.822343	38.191015
2071.949706	441980.910063	38.196032
2074.049444	442789.269317	38.201050
2076.107620	443597.403648	38.206068
2077.808931	444420.139092	38.211085
2080.532083	445228.407657	38.216103
2082.300381	446048.389620	38.221120
2084.787393	446870.347082	38.226138
2086.747035	447679.966177	38.231156
2088.804470	448503.450264	38.236173
2091.355839	449316.805600	38.241191
2093.183406	450131.261120	38.246208
2095.628986	450943.611005	38.251226
2097.519476	451766.491286	38.256244
2099.626322	452586.977358	38.261261
2102.069119	453390.483957	38.266279
2103.541665	454217.181228	38.271296
2106.159888	455039.510024	38.276314
2108.114651	455860.449219	38.281332
2110.032897	456693.700324	38.286349
2112.747179	457524.055978	38.291367
2114.335896	458345.209487	38.296384
2116.801642	459164.162957	38.301402
2118.718184	459998.190114	38.306420
2120.556471	460833.662031	38.311437
2122.612889	461652.784728	38.316455
2124.657996	462494.270837	38.321472
2126.662148	463337.497611	38.326490
2128.843227	464183.995751	38.331508
2130.924172	465025.975681	38.336525
2132.859564	465866.629603	38.341543
2135.386388	466728.327218	38.346560
2137.049735	467563.697009	38.351578
2139.179328	468421.089669	38.356596
2141.395860	469275.398050	38.361613
2143.772456	470123.325680	38.366631
2145.620705	470977.366851	38.371648
2147.857597	471798.664369	38.376666
2149.837093	472621.737482	38.381684
2151.498288	473455.841832	38.386701
2153.785217	474293.797571	38.391719
2155.811081	475127.515514	38.396736
2157.694079	475969.454455	38.401754
2159.934621	476812.963618	38.406772
2161.628470	477659.252517	38.411789
2164.127008	478502.794149	38.416807
2166.156709	479375.265490	38.421824
2168.204389	480224.510311	38.426842
2170.756505	481079.794138	38.431860
2173.093576	481951.132857	38.436877
2175.518264	482811.204694	38.441895
2177.470991	483683.382257	38.446912
2179.167520	484547.430436	38.451930
2181.362474	485425.290650	38.456948
2183.529768	486327.498678	38.461965
2186.112658	487213.436898	38.466983
2188.242666	488097.083391	38.472000
2190.355906	488980.486641	38.477018
2192.968806	489869.114036	38.482036
2195.039815	490751.223905	38.487053
2197.308859	491641.534378	38.492071
2199.312086	492548.599671	38.497088
2201.444610	493445.855818	38.502106
2203.890948	494336.402618	38.507124
2205.922719	495254.322877	38.512141
2208.207704	496159.688496	38.517159
2209.809103	497077.935186	38.522176
2212.124089	497988.093207	38.527194
2214.695975	498897.605021	38.532212
2216.845514	499836.701040	38.537229
2219.312194	500754.958639	38.542247
2221.430358	501686.086625	38.547264
2223.687255	502612.953139	38.552282
2226.068296	503543.681688	38.557300
2228.277080	504472.822796	38.562317
2230.572687	505411.025563	38.567335
2232.792285	506343.236528	38.572352
2234.791087	507292.475105	38.577370
2237.135066	508239.987893	38.582388
2238.756883	509188.522431	38.587405
2241.194992	510117.354880	38.592423
2243.733228	511074.501018	38.597440
2245.904783	512033.868622	38.602458
2247.816622	512979.913409	38.607476
2250.018812	513945.310856	38.612493
2252.195506	514911.712165	38.617511
2254.314048	515874.082305	38.622528
2256.628257	516843.517640	38.627546
2258.773238	517830.659460	38.632564
2261.115797	518808.635950	38.637581
2263.563392	519781.545219	38.642599
2265.743403	520761.592004	38.647616
2267.858788	521757.759425	38.652634
2270.586500	522736.632862	38.657652
2272.741876	523706.319491	38.662669
2275.485081	524686.878796	38.667687
2278.017311	525670.733820	38.672704
2279.907926	526650.248886	38.677722
2282.254152	527620.962973	38.682740
2284.159627	528617.067438	38.687757
2286.865499	529592.781295	38.692775
2289.069786	530575.059606	38.697792
2291.058354	531557.409141	38.702810
2293.374878	532537.222758	38.707828
2295.316664	533526.497143	38.712845
2298.103742	534488.936606	38.717863
2300.234555	535443.870656	38.722880
2302.461783	536398.575187	38.727898
2304.947118	537360.018967	38.732916
2307.134374	538321.699564	38.737933
2309.415259	539273.789757	38.742951
2311.625642	540243.439744	38.747968
2313.488534	541212.427183	38.752986
2315.999860	542178.374075	38.758004
2317.985401	543168.137503	38.763021
2319.932493	544148.078999	38.768039
2322.318532	545139.801261	38.773056
2324.479749	546140.141652	38.778074
2327.053815	547131.792553	38.783092
2328.720130	548137.804908	38.788109
2331.251260	549144.154968	38.793127
2334.016638	550165.327136	38.798144
2336.262753	551180.123859	38.803162
2338.914906	552191.259409	38.808180
2341.282456	553219.509708	38.813197
2343.703036	554236.112185	38.818215
2346.279096	555251.105041	38.823232
2348.185385	556276.133959	38.828250
2351.011521	557307.165096	38.833268
2353.070792	558344.625591	38.838285
2355.324675	559380.265175	38.843303
2358.214329	560416.322475	38.848320
2360.239352	561469.774535	38.853338
2362.500221	562500.547718	38.858356
2364.512314	563548.460949	38.863373
2366.900832	564599.644143	38.868391
2369.324723	565671.128288	38.873408
2371.823768	566733.723513	38.878426
2374.484285	567788.271112	38.883444
2376.542242	568859.301792	38.888461
2378.986618	569936.807354	38.893479
2381.409146	571016.083777	38.898496
2383.469776	572090.710609	38.903514
2385.927485	573157.953414	38.908532
2388.290702	574254.785134	38.913549
2390.543852	575340.197906	38.918567
2393.025950	576439.530679	38.923584
2395.353834	577544.462913	38.928602
2397.854559	578630.303692	38.933620
2400.217545	579720.738499	38.938637
2402.424778	580829.614195	38.943655
2404.933553	581938.792451	38.948672
2407.176232	583053.532411	38.953690
2409.656553	584159.506253	38.958708
2411.644984	585290.083375	38.963725
2414.204870	586416.701048	38.968743
2417.123935	587529.868876	38.973760
2419.518602	588655.503996	38.978778
2421.823598	589776.838309	38.983796
2424.578354	590899.397504	38.988813
2427.085202	592020.489208	38.993831
2429.599419	593145.884573	38.998848
2431.446552	594271.333690	39.003866
2434.024444	595400.814496	39.008884
2436.355456	596534.686976	39.013901
2438.882173	597665.913354	39.018919
2441.510989	598798.015703	39.023936
2443.725571	599940.895133	39.028954
2446.106659	601074.520507	39.033972
2448.550615	602220.193138	39.038989
2450.820792	603364.579329	39.044007
2452.809608	604501.238380	39.049024
2455.490721	605649.835523	39.054042
2458.023303	606772.012890	39.059060
2460.404843	607895.856560	39.064077
2462.789641	608998.319318	39.069095
2465.310319	610121.119020	39.074112
2467.311255	611257.802647	39.079130
2469.695169	612375.596964	39.084148
2472.091017	613507.785306	39.089165
2473.892520	614646.159475	39.094183
2476.800789	615789.436460	39.099200
2478.841255	616941.240444	39.104218
2481.312599	618087.652988	39.109236
2483.782205	619268.696269	39.114253
2486.554920	620430.114900	39.119271
2488.807955	621589.996303	39.124288
2490.848947	622768.733088	39.129306
2493.898124	623966.817218	39.134324
2495.839952	625157.255615	39.139341
2498.414142	626351.106082	39.144359
2501.129429	627547.898382	39.149376
2503.640510	628757.179542	39.154394
2506.509568	629957.423615	39.159412
2508.947283	631178.230444	39.164429
2511.151760	632380.457909	39.169447
2514.150968	633592.504060	39.174464
2516.725317	634813.966882	39.179482
2519.526763	636030.607406	39.184500
2522.301756	637250.804468	39.189517
2525.023494	638453.099574	39.194535
2527.983658	639663.899440	39.199552
2530.279932	640885.145635	39.204570
2532.799075	642102.967484	39.209588
2535.186876	643330.743659	39.214605
2537.262119	644554.383868	39.219623
2539.980324	645788.344699	39.224640
2542.114197	647038.209874	39.229658
2544.741908	648283.850561	39.234676
2547.133368	649538.898962	39.239693
2549.283562	650788.895517	39.244711
2551.918472	652047.877354	39.249728
2554.432240	653330.841541	39.254746
2557.008082	654598.132949	39.259764
2559.668999	655869.533330	39.264781
2561.974085	657153.831246	39.269799
2564.725398	658422.994698	39.274816
2567.084039	659712.229653	39.279834
2569.497743	660998.845541	39.284852
2572.224897	662283.497261	39.289869
2574.654886	663590.680131	39.294887
2577.584785	664891.431614	39.299904
2580.249572	666188.517611	39.304922
2582.790566	667483.259332	39.309940
2585.221624	668786.750806	39.314957
2587.218303	670107.747702	39.319975
2590.230562	671419.589060	39.324992
2592.792536	672730.726193	39.330010
2595.326580	674038.552902	39.335028
2598.160574	675364.148251	39.340045
2600.781267	676688.099891	39.345063
2603.235954	677999.861711	39.350080
2605.943033	679316.019468	39.355098
2608.311536	680646.656716	39.360116
2611.147290	681974.789548	39.365133
2613.736399	683316.582843	39.370151
2616.376110	684645.852749	39.375168
2618.558488	685980.418571	39.380186
2620.980013	687304.122689	39.385204
2624.011951	688649.131873	39.390221
2626.696065	689974.587717	39.395239
2629.185886	691276.501871	39.400256
2632.137992	692573.486186	39.405274
2634.479318	693868.497855	39.410292
2637.417484	695161.834238	39.415309
2640.030259	696460.443724	39.420327
2642.470347	697747.830633	39.425344
2645.269419	699052.080931	39.430362
2647.808672	700344.776231	39.435380
2651.031179	701645.745986	39.440397
2653.379799	702948.004973	39.445415
2656.250995	704256.278282	39.450432
2659.100824	705566.538921	39.455450
2661.643016	706858.665870	39.460468
2664.314781	708177.925538	39.465485
2666.733365	709496.925885	39.470503
2669.736840	710803.196055	39.475520
2672.120453	712123.779131	39.480538
2674.531866	713455.045765	39.485556
2676.988868	714787.730123	39.490573
2679.931048	716120.768438	39.495591
2682.861797	717449.985661	39.500608
2685.596811	718803.814867	39.505626
2688.419197	720143.311728	39.510644
2691.109903	721492.607562	39.515661
2693.477261	722847.623607	39.520679
2696.256069	724200.719121	39.525696
2698.801597	725548.638587	39.530714
2701.217258	726935.707097	39.535732
2704.327051	728304.882075	39.540749
2706.556235	729682.127067	39.545767
2709.661333	731063.343441	39.550784
2712.189198	732443.531561	39.555802
2714.838911	733840.405729	39.560820
2717.548555	735221.868795	39.565837
2720.160932	736636.240451	39.570855
2723.231948	738038.341532	39.575872
2725.776733	739451.635676	39.580890
2728.182662	740856.165562	39.585908
2731.582390	742255.201954	39.590925
2734.210769	743676.514120	39.595943
2737.050510	745082.789106	39.600960
2739.610660	746507.055091	39.605978
2743.101709	747921.443229	39.610996
2745.121682	749326.895983	39.616013
2747.987249	750761.822708	39.621031
2750.719717	752175.515102	39.626048
2753.483469	753606.187710	39.631066
2756.221721	755037.781646	39.636084
2759.098362	756474.060565	39.641101
2761.675292	757906.328554	39.646119
2764.695416	759333.036851	39.651136
2767.463047	760770.052822	39.656154
2770.120086	762214.196806	39.661172
2773.059125	763651.770202	39.666189
2775.665043	765096.306665	39.671207
2778.249251	766539.093750	39.676224
2781.112074	767994.096406	39.681242
2783.334518	769431.615563	39.686260
2786.396928	770895.802778	39.691277
2788.804123	772363.986354	39.696295
2792.039739	773833.854794	39.701312
2794.740881	775286.619264	39.706330
2797.426823	776759.432675	39.711348
2800.650461	778223.955350	39.716365
2802.971415	779695.844504	39.721383
2806.372942	781151.845007	39.726400
2808.982286	782616.124672	39.731418
2811.494995	784070.065171	39.736436
2814.657507	785513.009124	39.741453
2816.942559	786929.028578	39.746471
2819.813245	788343.935900	39.751488
2822.584025	789778.631017	39.756506
2825.507011	791206.590501	39.761524
2828.350526	792630.845029	39.766541
2830.713688	794080.811072	39.771559
2833.507220	795517.181425	39.776576
2836.343832	796974.457830	39.781594
2838.553339	798426.245882	39.786612
2841.638707	799877.440765	39.791629
2844.423866	801360.539830	39.796647
2847.183741	802838.040853	39.801664
2849.807738	804312.655429	39.806682
2852.311117	805804.779106	39.811700
2855.471471	807293.829555	39.816717
2857.960118	808802.468401	39.821735
2860.890684	810323.996781	39.826752
2863.412182	811846.571673	39.831770
2866.268135	813365.231557	39.836788
2869.193889	814891.305569	39.841805
2871.931551	816443.876678	39.846823
2874.855489	817983.656058	39.851840
2878.022912	819532.169335	39.856858
2880.545074	821087.505833	39.861876
2883.495858	822641.383074	39.866893
2886.002833	824207.749474	39.871911
2889.007383	825798.827094	39.876928
2892.224391	827379.733487	39.881946
2894.975211	828965.258822	39.886964
2897.985426	830560.152208	39.891981
2900.281053	832154.334312	39.896999
2903.079884	833764.116192	39.902016
2905.917347	835364.871730	39.907034
2908.938162	837003.320128	39.912052
2911.851663	838606.908153	39.917069
2914.707614	840238.667857	39.922087
2917.531929	841874.442560	39.927104
2920.650840	843513.444347	39.932122
2923.205280	845154.060265	39.937140
2926.319721	846789.685743	39.942157
2929.387057	848446.276920	39.947175
2932.159617	850106.463212	39.952192
2935.295198	851754.491730	39.957210
2938.042922	853421.668903	39.962228
2941.156565	855080.279669	39.967245
2944.311084	856747.466258	39.972263
2947.104969	858406.013313	39.977280
2950.006533	860071.856152	39.982298
2952.904556	861750.824645	39.987316
2956.121775	863417.643690	39.992333
2959.115961	865102.653913	39.997351
2961.702426	866776.506531	40.002368
2965.185920	868442.094287	40.007386
2968.019347	870133.091093	40.012404
2970.957235	871808.005512	40.017421
2973.700614	873486.451678	40.022439
2976.797513	875177.527762	40.027456
2980.015681	876863.168627	40.032474
2982.877788	878548.388235	40.037492
2985.905855	880234.259464	40.042509
2989.414649	881908.838967	40.047527
2992.731220	883590.315666	40.052544
2995.862903	885275.685945	40.057562
2998.488415	886963.645547	40.062580
3001.641502	888636.351906	40.067597
3004.353304	890314.438308	40.072615
3006.969508	891982.692175	40.077632
3010.675973	893624.140160	40.082650
3013.279900	895263.756161	40.087668
3016.467165	896889.886200	40.092685
3019.352732	898507.890545	40.097703
3021.994277	900143.202555	40.102720
3025.052807	901783.944954	40.107738
3027.721371	903434.481319	40.112756
3030.698295	905090.161662	40.117773
3033.870664	906735.407257	40.122791
3036.414902	908397.396947	40.127808
3039.637209	910070.993529	40.132826
3042.213204	911740.056634	40.137844
3045.205117	913423.734760	40.142861
3047.881024	915115.983124	40.147879
3050.746945	916833.039699	40.152896
3053.977182	918525.200421	40.157914
3057.094626	920255.352587	40.162932
3059.767026	921963.145041	40.167949
3062.724084	923696.161074	40.172967
3065.652077	925425.844034	40.177984
3068.855952	927166.431284	40.183002
3071.846754	928926.137951	40.188020
3074.783036	930685.944851	40.193037
3077.860948	932452.522507	40.198055
3081.006199	934229.129864	40.203072
3083.935396	935997.135363	40.208090
3086.752077	937791.933891	40.213108
3090.171345	939583.915512	40.218125
3093.049781	941386.274028	40.223143
3095.900973	943181.227420	40.228160
3099.463732	944989.873260	40.233178
3102.417753	946808.591259	40.238196
3105.451193	948621.976543	40.243213
3108.748278	950437.924902	40.248231
3111.565601	952272.489285	40.253248
3114.430687	954107.054946	40.258266
3117.489156	955980.359647	40.263284
3120.718783	957880.214138	40.268301
3123.295449	959789.622072	40.273319
3126.391079	961707.598276	40.278336
3129.792206	963606.124731	40.283354
3132.653087	965533.125424	40.288372
3135.732647	967466.768176	40.293389
3138.993414	969396.802027	40.298407
3141.791203	971339.729771	40.303424
3145.369292	973273.286634	40.308442
3148.306638	975227.360264	40.313460
3151.335805	977178.509899	40.318477
3155.021780	979117.386879	40.323495
3157.827030	981080.300245	40.328512
3161.263709	983031.333316	40.333530
3164.403079	984986.031619	40.338548
3167.571878	986934.702451	40.343565
3170.878046	988894.163360	40.348583
3173.664349	990867.914337	40.353600
3177.114087	992832.510324	40.358618
3180.082204	994803.891961	40.363636
3182.981011	996772.657267	40.368653
3186.097300	998742.839675	40.373671
3188.906741	1000744.715151	40.378688
3192.356040	1002739.081005	40.383706
3195.514964	1004737.253743	40.388724
3198.409976	1006734.278279	40.393741
3201.552113	1008729.198299	40.398759
3204.685808	1010743.570858	40.403776
3207.710940	1012748.038000	40.408794
3210.727642	1014757.602989	40.413812
3213.533469	1016761.160264	40.418829
3216.889943	1018740.784171	40.423847
3219.637027	1020721.261205	40.428864
3223.115415	1022692.988703	40.433882
3225.956750	1024675.533944	40.438900
3229.271886	1026647.732123	40.443917
3232.780627	1028631.277742	40.448935
3235.762416	1030618.358129	40.453952
3238.982983	1032616.082366	40.458970
3242.257635	1034607.581659	40.463988
3245.095929	1036613.488873	40.469005
3248.209143	1038629.041939	40.474023
3251.238169	1040656.987485	40.479040
3254.595099	1042690.883609	40.484058
3257.869579	1044731.946171	40.489076
3261.045045	1046781.805852	40.494093
3264.182276	1048841.211879	40.499111
3267.175813	1050903.146386	40.504128
3270.703488	1052957.683784	40.509146
3273.526991	1055037.434879	40.514164
3276.959532	1057122.740773	40.519181
3280.307915	1059213.227818	40.524199
3283.181877	1061326.431107	40.529216
3286.403710	1063415.438589	40.534234
3289.225210	1065538.358854	40.539252
3292.489295	1067660.097590	40.544269
3295.790792	1069794.720694	40.549287
3299.110595	1071953.908280	40.554304
3302.515901	1074094.505488	40.559322
3305.506786	1076251.858903	40.564340
3308.553451	1078415.435277	40.569357
3312.187663	1080587.722133	40.574375
3315.308037	1082776.158978	40.579392
3318.442885	1084955.203943	40.584410
3321.559804	1087156.031184	40.589428
3324.738221	1089369.428053	40.594445
3328.344729	1091571.537733	40.599463
3331.818235	1093780.125530	40.604480
3335.173046	1095982.297731	40.609498
3339.015137	1098198.945642	40.614516
3342.219258	1100415.647585	40.619533
3345.752608	1102635.006840	40.624551
3348.812141	1104854.674047	40.629568
3352.622620	1107065.875360	40.634586
3355.925124	1109296.526867	40.639604
3359.101265	1111520.279277	40.644621
3363.092603	1113743.927700	40.649639
3366.159612	1115982.112765	40.654656
3369.321354	1118204.712811	40.659674
3372.859223	1120439.531750	40.664692
3375.969360	1122671.208248	40.669709
3379.535916	1124893.240252	40.674727
3383.061217	1127139.494564	40.679744
3386.331532	1129365.688190	40.684762
3390.118530	1131601.198146	40.689780
3393.199293	1133832.568322	40.694797
3396.744139	1136063.303681	40.699815
3399.717879	1138312.697787	40.704832
3402.917256	1140568.954664	40.709850
3406.175855	1142812.605616	40.714868
3409.459300	1145064.755841	40.719885
3412.903715	1147311.571994	40.724903
3415.891448	1149597.940113	40.729920
3419.041722	1151869.408768	40.734938
3422.003409	1154135.209212	40.739956
3425.177062	1156421.793071	40.744973
3428.804941	1158709.476020	40.749991
3431.818298	1161014.550340	40.755008
3435.406623	1163286.466767	40.760013
3438.428898	1165514.494901	40.765018
3441.655000	1167706.901066	40.770023
3444.880536	1169813.664138	40.775028
3448.012062	1171859.611242	40.780032
3450.885496	1173823.533774	40.785037
3453.896695	1175716.861393	40.790042
3456.820487	1177551.106335	40.795047
3460.160732	1179287.917923	40.800052
3462.505287	1180964.248285	40.805056
3464.924778	1182559.179509	40.810061
3467.726952	1184087.883699	40.815066
3470.073132	1185534.378324	40.820071
3472.459052	1186896.863536	40.825076
3474.554529	1188212.783249	40.830080
3476.611110	1189426.770550	40.835085
3478.953508	1190588.178245	40.840090
3481.186431	1191690.154323	40.845095
3483.019874	1192723.297339	40.850100
3484.599306	1193702.369043	40.855104
3486.584522	1194614.897047	40.860109
3488.698768	1195479.832313	40.865114
3490.207792	1196287.651377	40.870119
3491.960162	1197010.085365	40.875124
3493.148984	1197710.364377	40.880128
3494.347058	1198344.303604	40.885133
3496.157328	1198955.547600	40.890138
3496.852695	1199507.522442	40.895143
3498.440436	1200009.765553	40.900148
3499.624141	1200487.265584	40.905152
3500.474331	1200918.541751	40.910157
3501.856308	1201311.246519	40.915162
3502.452935	1201661.854883	40.920167
3503.817598	1201996.091935	40.925172
3504.240329	1202289.584387	40.930176
3505.410733	1202536.717095	40.935181
3506.497366	1202768.476976	40.940186
3507.262711	1202969.156141	40.945191
3507.890756	1203136.103175	40.950196
3508.913818	1203281.326055	40.955200
3509.346963	1203383.054379	40.960205
3510.096919	1203479.479330	40.965210
3510.520639	1203559.177846	40.970215
3511.272078	1203607.889343	40.975220
3511.446052	1203628.575756	40.980224
3512.158245	1203647.111336	40.985229
3512.989409	1203644.068856	40.990234
3513.110992	1203618.178738	40.995239
3513.479365	1203566.471120	41.000244
3513.604942	1203516.208988	41.005248
3514.149109	1203461.190644	41.010253
3514.640621	1203369.810413	41.015258
3515.173080	1203258.267879	41.020263
3515.755288	1203155.432680	41.025268
3515.458665	1203027.710671	41.030272
3515.865930	1202887.307587	41.035277
3516.301915	1202733.489850	41.040282
3516.467332	1202584.587158	41.045287
3516.743603	1202417.567258	41.050292
3517.172387	1202244.235034	41.055296
3517.227400	1202063.363866	41.060301
3517.452425	1201857.516907	41.065306
3517.577656	1201650.084067	41.070311
3517.846956	1201432.772999	41.075316
3517.920908	1201218.298213	41.080320
3518.245908	1201000.021908	41.085325
3518.554068	1200768.327892	41.090330
3518.473810	1200541.470643	41.095335
3518.807658	1200279.362636	41.100340
3518.963110	1200041.189226	41.105344
3518.898440	1199779.590366	41.110349
3519.284744	1199524.376650	41.115354
3518.944199	1199246.285935	41.120359
3519.439065	1198986.243197	41.125364
3519.296713	1198713.438618	41.130368
3519.361769	1198433.266876	41.135373
3519.838425	1198150.103284	41.140378
3519.663810	1197874.163040	41.145383
3519.623771	1197576.226603	41.150388
3519.702143	1197280.787328	41.155392
3519.872311	1196984.002028	41.160397
3520.033645	1196695.366830	41.165402
3520.081040	1196390.589521	41.170407
3520.312307	1196078.442012	41.175412
3520.184823	1195777.224285	41.180416
3519.867015	1195471.232337	41.185421
3520.255330	1195155.060003	41.190426
3520.368310	1194851.025800	41.195431
3520.305790	1194526.626603	41.200436
3520.534244	1194210.234856	41.205440
3520.626004	1193886.333393	41.210445
3520.468627	1193562.358699	41.215450
3520.462912	1193242.846935	41.220455
3520.665386	1192904.965133	41.225460
3520.655129	1192576.959337	41.230464
3520.474310	1192249.900180	41.235469
3520.799780	1191907.893418	41.240474
3520.177529	1191587.159359	41.245479
3520.610384	1191246.030591	41.250484
3520.658668	1190915.372686	41.255488
3520.633959	1190570.985937	41.260493
3520.579867	1190235.132956	41.265498
3520.593841	1189900.186760	41.270503
3520.812096	1189546.575367	41.275508
3520.417749	1189216.539543	41.280512
3520.501217	1188880.011858	41.285517
3520.724078	1188544.285378	41.290522
3520.770541	1188203.301391	41.295527
3520.556603	1187848.892944	41.300532
3520.672487	1187497.602793	41.305536
3520.813475	1187160.295541	41.310541
3521.016600	1186809.978701	41.315546
3520.511421	1186460.413117	41.320551
3520.656981	1186109.964332	41.325556
3520.775403	1185768.243692	41.330560
3521.033338	1185420.269287	41.335565
3521.229002	1185057.700801	41.340570
3520.563063	1184713.217593	41.345575
3520.815473	1184355.294451	41.350580
3521.048288	1183994.997565	41.355584
3520.930117	1183626.358825	41.360589
3520.867799	1183279.422536	41.365594
3520.354889	1182922.938064	41.370599
3520.699527	1182564.970219	41.375604
3520.553321	1182216.564881	41.380608
3520.684575	1181878.632854	41.385613
3520.784323	1181505.665783	41.390618
3520.439867	1181163.529432	41.395623
3520.595277	1180795.868244	41.400628
3520.844395	1180447.184833	41.405632
3520.387647	1180083.151855	41.410637
3520.588404	1179725.953468	41.415642
3520.144309	1179374.487159	41.420647
3520.576312	1179004.864297	41.425652
3520.462462	1178652.918053	41.430656
3520.418352	1178293.777776	41.435661
3520.375007	1177939.039956	41.440666
3520.064466	1177584.133516	41.445671
3520.512296	1177230.114289	41.450676
3520.475342	1176871.910938	41.455680
3520.151102	1176526.639149	41.460685
3520.383340	1176150.533120	41.465690
3520.291019	1175811.771948	41.470695
3520.185293	1175450.466404	41.475700
3520.188565	1175096.092440	41.480704
3520.275327	1174725.468215	41.485709
3520.258425	1174371.236748	41.490714
3519.768747	1174029.314263	41.495719
3520.131760	1173678.178292	41.500724
3520.164218	1173315.570497	41.505728
3519.800457	1172967.051950	41.510733
3520.032771	1172612.094061	41.515738
3519.990460	1172256.780018	41.520743
3520.020999	1171890.867104	41.525748
3520.312652	1171541.202169	41.530752
3519.782548	1171186.933017	41.535757
3519.920469	1170829.416928	41.540762
3519.657847	1170476.187384	41.545767
3519.903153	1170108.416005	41.550772
3519.799885	1169761.715762	41.555776
3520.112166	1169413.508736	41.560781
3520.180166	1169032.386774	41.565786
3519.820821	1168679.806448	41.570791
3519.796551	1168314.501004	41.575796
3519.636082	1167976.940306	41.580800
3519.480867	1167620.951555	41.585805
3519.421970	1167275.400308	41.590810
3519.456628	1166918.954887	41.595815
3519.529591	1166556.814498	41.600820
3519.686496	1166215.028244	41.605824
3519.605799	1165854.091844	41.610829
3519.576182	1165496.238143	41.615834
3519.391548	1165151.133725	41.620839
3519.269805	1164795.796917	41.625844
3519.430619	1164439.256110	41.630848
3519.129055	1164094.667919	41.635853
3519.393769	1163750.813884	41.640858
3519.160988	1163402.768374	41.645863
3519.031830	1163047.219591	41.650868
3518.930433	1162711.765368	41.655872
3519.003218	1162358.403968	41.660877
3519.458030	1162009.491240	41.665882
3519.139166	1161657.753379	41.670887
3518.992556	1161308.042546	41.675892
3519.344218	1160964.936302	41.680896
3518.910134	1160616.360742	41.685901
3519.093440	1160259.437130	41.690906
3518.852719	1159909.364922	41.695911
3519.310031	1159557.641870	41.700916
3518.902102	1159226.363477	41.705920
3518.662170	1158884.258452	41.710925
3519.066304	1158530.017125	41.715930
3518.604798	1158187.997747	41.720935
3518.730954	1157831.958513	41.725940
3518.966917	1157486.847122	41.730944
3518.563002	1157142.953342	41.735949
3518.543811	1156800.392403	41.740954
3518.582322	1156457.421268	41.745959
3518.497923	1156122.393891	41.750964
3518.405172	1155792.171126	41.755968
3518.508685	1155445.906862	41.760973
3518.519286	1155101.716564	41.765978
3518.555209	1154763.649767	41.770983
3518.226716	1154426.851369	41.775988
3518.219791	1154077.487180	41.780992
3518.252239	1153735.853539	41.785997
3518.292172	1153401.200066	41.791002
3518.022347	1153068.090706	41.796007
3518.167959	1152718.232534	41.801012
3518.259337	1152389.374868	41.806016
3517.739226	1152046.870617	41.811021
3517.965898	1151728.268105	41.816026
3517.852923	1151389.440952	41.821031
3517.367572	1151060.027159	41.826036
3517.556730	1150739.382618	41.831040
3517.783466	1150408.579830	41.836045
3517.794294	1150074.193131	41.841050
3517.568781	1149752.136271	41.846055
3517.462555	1149427.293365	41.851060
3517.810818	1149096.198769	41.856064
3517.544341	1148761.300851	41.861069
3517.737122	1148431.895233	41.866074
3517.390043	1148103.979029	41.871079
3517.339939	1147781.772913	41.876084
3517.342176	1147444.378512	41.881088
3517.273904	1147125.167293	41.886093
3516.894863	1146811.010304	41.891098
3516.910228	1146492.978971	41.896103
3516.864841	1146158.068895	41.901108
3517.171154	1145848.006511	41.906112
3516.962752	1145542.560340	41.911117
3517.194467	1145223.184710	41.916122
3517.004936	1144894.379577	41.921127
3517.030189	1144579.359638	41.926132
3517.053427	1144263.467988	41.931136
3516.861415	1143933.845034	41.936141
3516.960072	1143613.919995	41.941146
3516.675379	1143315.469030	41.946151
3516.781018	1142987.255218	41.951156
3516.341840	1142667.076974	41.956160
3516.215124	1142360.864405	41.961165
3516.275004	1142044.739308	41.966170
3516.291587	1141754.307443	41.971175
3516.502648	1141442.674382	41.976180
3516.366378	1141130.985315	41.981184
3516.386902	1140829.023556	41.986189
3516.460757	1140521.817712	41.991194
3516.082389	1140210.588693	41.996199
3516.382929	1139892.587586	42.001204
3516.478031	1139577.068396	42.006208
3516.480934	1139269.422027	42.011213
3516.432016	1138960.152992	42.016218
3515.757149	1138654.290764	42.021223
3515.760794	1138353.044780	42.026228
3516.028423	1138039.114031	42.031232
3515.632195	1137755.934489	42.036237
3516.038204	1137442.989819	42.041242
3515.850182	1137146.263437	42.046247
3515.753905	1136843.334240	42.051252
3515.718750	1136554.429592	42.056256
3515.497540	1136255.000344	42.061261
3515.781542	1135946.355209	42.066266
3515.630386	1135651.343295	42.071271
3515.547072	1135358.867908	42.076276
3515.534859	1135069.878653	42.081280
3515.488872	1134761.408912	42.086285
3515.814890	1134471.856520	42.091290
3515.655948	1134177.523841	42.096295
3515.502279	1133869.969932	42.101300
3515.446736	1133582.521755	42.106304
3515.269300	1133292.988022	42.111309
3515.480692	1132994.918685	42.116314
3515.639629	1132696.841273	42.121319
3515.363208	1132391.122257	42.126324
3515.436925	1132111.934973	42.131328
3515.110124	1131820.730207	42.136333
3515.343691	1131522.099491	42.141338
3515.131534	1131235.785639	42.146343
3515.169277	1130933.257459	42.151348
3515.036916	1130659.825668	42.156352
3515.493501	1130368.697526	42.161357
3515.281008	1130066.541502	42.166362
3515.079506	1129789.273912	42.171367
3515.255777	1129493.390752	42.176372
3515.329984	1129198.743957	42.181376
3515.124990	1128911.067822	42.186381
3514.890027	1128628.896122	42.191386
3514.883659	1128340.871207	42.196391
3515.145284	1128032.435741	42.201396
3515.305698	1127758.616498	42.206400
3514.991117	1127467.551848	42.211405
3515.352654	1127179.784005	42.216410
3514.573714	1126891.998222	42.221415
3514.587428	1126601.022405	42.226420
3515.030699	1126329.080717	42.231424
3514.473503	1126035.028811	42.236429
3514.660935	1125745.785242	42.241434
3514.674618	1125474.156129	42.246439
3514.564234	1125183.789417	42.251444
3514.615397	1124902.800487	42.256448
3514.644704	1124634.646731	42.261453
3514.575317	1124343.656593	42.266458
3514.722881	1124079.166821	42.271463
3514.652788	1123789.574113	42.276468
3514.588893	1123511.195713	42.281472
3514.681067	1123220.403268	42.286477
3514.760434	1122936.260294	42.291482
3514.435551	1122660.165031	42.296487
3514.436447	1122368.008499	42.301492
3514.112953	1122085.885803	42.306496
3514.394561	1121824.689617	42.311501
3514.521423	1121542.178417	42.316506
3514.087808	1121261.077647	42.321511
3513.886971	1120982.494778	42.326516
3513.903766	1120716.622115	42.331520
3513.893309	1120447.883735	42.336525
3514.246081	1120162.595901	42.341530
3514.061276	1119907.478078	42.346535
3513.743484	1119640.273607	42.351540
3513.825527	1119359.273636	42.356544
3513.890317	1119087.406432	42.361549
3513.917590	1118819.723113	42.366554
3513.790377	1118557.482039	42.371559
3513.706529	1118281.216098	42.376564
3513.938331	1118019.270612	42.381568
3513.361871	1117759.351041	42.386573
3513.652156	1117490.890984	42.391578
3513.671252	1117234.945139	42.396583
3513.326721	1116969.993960	42.401588
3513.563813	1116698.072317	42.406592
3513.343573	1116444.319995	42.411597
3513.587786	1116183.521629	42.416602
3513.669607	1115931.315512	42.421607
3513.394886	1115659.044180	42.426612
3513.257154	1115393.123079	42.431616
3513.107751	1115138.344010	42.436621
3512.899065	1114879.844652	42.441626
3513.336210	1114619.129060	42.446631
3513.050325	1114362.142840	42.451636
3513.331679	1114112.773872	42.456640
3513.229136	1113850.774982	42.461645
3513.235897	1113587.028905	42.466650
3512.996627	1113340.856511	42.471655
3513.010024	1113070.980977	42.476660
3513.376973	1112823.731378	42.481664
3512.861055	1112577.092659	42.486669
3513.227893	1112332.300137	42.491674
3513.054228	1112063.263135	42.496679
3512.855170	1111800.321578	42.501684
3513.003092	1111548.375374	42.506688
3512.957953	1111294.255049	42.511693
3512.789631	1111043.291190	42.516698
3512.807071	1110801.634644	42.521703
3512.598637	1110541.781347	42.526708
3512.581416	1110294.096912	42.531712
3512.413313	1110056.540182	42.536717
3512.480286	1109803.285035	42.541722
3512.016542	1109557.739482	42.546727
3512.373536	1109321.972330	42.551732
3512.204841	1109086.949464	42.556736
3512.333324	1108843.850500	42.561741
3512.609953	1108591.171800	42.566746
3511.909046	1108361.549713	42.571751
3511.969329	1108123.010884	42.576756
3512.373948	1107885.072960	42.581760
3511.945826	1107637.238321	42.586765
3511.901228	1107399.639297	42.591770
3512.078611	1107180.896040	42.596775
3511.928449	1106943.962562	42.601780
3512.452564	1106696.023212	42.606784
3512.085500	1106468.843209	42.611789
3512.306069	1106233.727037	42.616794
3511.970985	1105996.686831	42.621799
3511.575727	1105751.720103	42.626804
3511.973286	1105518.262435	42.631808
3511.743733	1105300.560280	42.636813
3512.018899	1105054.018869	42.641818
3511.909473	1104821.760596	42.646823
3511.774118	1104583.001584	42.651828
3511.971190	1104349.144224	42.656832
3512.080490	1104120.067320	42.661837
3512.090365	1103880.393555	42.666842
3512.044982	1103657.722792	42.671847
3511.849119	1103434.112263	42.676852
3511.765595	1103190.410728	42.681856
3511.420190	1102961.168384	42.686861
3511.562584	1102726.103100	42.691866
3511.621803	1102501.934159	42.696871
3511.327612	1102270.647438	42.701876
3511.628455	1102043.744105	42.706880
3511.740596	1101825.080781	42.711885
3511.791399	1101581.284410	42.716890
3511.671133	1101352.701155	42.721895
3511.527764	1101124.781053	42.726900
3511.665080	1100898.716696	42.731904
3511.510981	1100673.646708	42.736909
3511.514210	1100435.541451	42.741914
3511.290648	1100222.508186	42.746919
3511.398859	1099999.661103	42.751924
3511.537159	1099773.740675	42.756928
3510.997316	1099554.901562	42.761933
3511.225803	1099322.828778	42.766938
3510.816054	1099118.482925	42.771943
3511.123714	1098894.983749	42.776948
3511.169260	1098670.275450	42.781952
3511.292978	1098462.852735	42.786957
3511.330799	1098233.824522	42.791962
3511.036119	1098026.836490	42.796967
3510.848992	1097790.654232	42.801972
3510.888849	1097570.969815	42.806977
3510.651493	1097369.685500	42.811981
3510.949279	1097145.446120	42.816986
3510.793351	1096931.984998	42.821991
3511.053898	1096709.551035	42.826996
3511.138769	1096498.520153	42.832001
3510.725101	1096285.075945	42.837005
3510.672650	1096064.293248	42.842010
3510.740591	1095858.310448	42.847015
3510.607225	1095651.874599	42.852020
3510.673660	1095430.185394	42.857025
3510.597480	1095221.810186	42.862029
3510.709253	1095008.611795	42.867034
3510.611873	1094813.715817	42.872039
3510.563351	1094600.719139	42.877044
3510.725286	1094387.392334	42.882049
3510.302160	1094186.977121	42.887053
3510.663596	1093980.108922	42.892058
3510.162127	1093759.401852	42.897063
3510.206949	1093552.473762	42.902068
3510.349251	1093353.848784	42.907073
3510.209106	1093155.071610	42.912077
3510.311919	1092950.216739	42.917082
3510.353354	1092761.828759	42.922087
3510.083891	1092539.214998	42.927092
3510.639848	1092333.592096	42.932097
3510.513885	1092138.508819	42.937101
3510.225582	1091932.339602	42.942106
3509.744448	1091730.215468	42.947111
3509.468257	1091523.358501	42.952116
3509.807735	1091328.169402	42.957121
3509.872747	1091150.828442	42.962125
3509.917927	1090935.182644	42.967130
3510.151867	1090747.171728	42.972135
3509.982873	1090561.040152	42.977140
3510.223256	1090354.436569	42.982145
3509.821573	1090150.325117	42.987149
3510.029285	1089945.147882	42.992154
3509.904192	1089753.330718	42.997159
3509.855023	1089569.444031	43.002164
3510.169001	1089374.955115	43.007169
3509.747138	1089178.856256	43.012173
3509.760137	1088975.015438	43.017178
3509.743397	1088783.529314	43.022183
3509.543696	1088588.330468	43.027188
3509.560017	1088410.524773	43.032193
3509.441305	1088211.658620	43.037197
3509.581266	1088014.946157	43.042202
3509.382199	1087836.773920	43.047207
3509.478358	1087648.870000	43.052212
3509.798939	1087462.359882	43.057217
3509.313836	1087280.000523	43.062221
3509.664686	1087083.602890	43.067226
3509.617922	1086892.150850	43.072231
3509.505587	1086699.648725	43.077236
3509.981540	1086508.288736	43.082241
3509.265673	1086327.277077	43.087245
3509.503219	1086143.610505	43.092250
3509.343025	1085953.965068	43.097255
3509.315437	1085757.006774	43.102260
3509.474703	1085580.426780	43.107265
3509.388430	1085404.360760	43.112269
3509.622990	1085204.942956	43.117274
3509.371312	1085013.937797	43.122279
3509.156853	1084849.282311	43.127284
3509.152579	1084657.552845	43.132289
3508.917234	1084484.645205	43.137293
3509.075693	1084280.508422	43.142298
3509.312327	1084100.512075	43.147303
3509.052314	1083929.987785	43.152308
3509.232800	1083748.071437	43.157313
3508.801016	1083570.948263	43.162317
3509.107314	1083378.930822	43.167322
3509.160453	1083222.524394	43.172327
3508.846578	1083030.596809	43.177332
3508.896347	1082849.535023	43.182337
3508.987702	1082678.721859	43.187341
3509.053368	1082506.277188	43.192346
3508.980713	1082316.778231	43.197351
3508.839093	1082137.258814	43.202356
3509.111903	1081959.679425	43.207361
3508.919741	1081787.734040	43.212365
3508.941687	1081617.762292	43.217370
3509.143427	1081420.321480	43.222375
3508.762118	1081241.291629	43.227380
3508.764212	1081069.675293	43.232385
3508.549074	1080904.420907	43.237389
3508.757214	1080726.716059	43.242394
3508.880457	1080554.679811	43.247399
3508.620612	1080384.236301	43.252404
3508.687730	1080200.109392	43.257409
3508.604276	1080044.305815	43.262413
3508.834901	1079869.159912	43.267418
3508.785965	1079704.225567	43.272423
3508.872671	1079531.299461	43.277428
3508.510391	1079345.679106	43.282433
3508.323659	1079173.362446	43.287437
3508.695680	1079007.665960	43.292442
3508.747433	1078836.355006	43.297447
3508.350640	1078664.440740	43.302452
3508.323681	1078489.101005	43.307457
3508.458800	1078331.772870	43.312461
3508.427908	1078171.876056	43.317466
3508.472813	1078003.419507	43.322471
3508.136478	1077838.668050	43.327476
3508.592582	1077671.477350	43.332481
3508.430627	1077503.807370	43.337485
3508.288404	1077333.057125	43.342490
3508.352069	1077164.955593	43.347495
3508.245147	1077000.237039	43.352500
3508.527630	1076836.121413	43.357505
3508.112656	1076679.988325	43.362509
3508.525536	1076504.704416	43.367514
3508.602688	1076335.134965	43.372519
3508.230003	1076175.427990	43.377524
3508.267603	1076012.480144	43.382529
3507.978378	1075845.356302	43.387533
3508.079889	1075667.984350	43.392538
3508.027867	1075516.559464	43.397543
3508.103243	1075364.725277	43.402548
3508.329753	1075205.947599	43.407553
3508.208116	1075038.675445	43.412557
3508.194435	1074870.035843	43.417562
3507.941526	1074704.791907	43.422567
3508.173955	1074560.592867	43.427572
3508.214781	1074391.449301	43.432577
3508.029422	1074227.524475	43.437581
3508.018877	1074067.215962	43.442586
3507.972926	1073912.479824	43.447591
3507.962864	1073746.206353	43.452596
3507.870327	1073584.552371	43.457601
3507.847357	1073446.994280	43.462605
3507.974912	1073286.736207	43.467610
3507.877194	1073129.008353	43.472615
3507.780169	1072977.424466	43.477620
3507.664297	1072816.135903	43.482625
3507.850976	1072662.767220	43.487629
3507.709111	1072508.487545	43.492634
3507.764763	1072362.338057	43.497639
3507.669147	1072206.985350	43.502644
3508.062929	1072048.857149	43.507649
3507.620292	1071903.257911	43.512653
3507.556986	1071747.022004	43.517658
3507.805232	1071597.168797	43.522663
3507.589988	1071429.801652	43.527668
3507.680202	1071293.420067	43.532673
3507.681340	1071146.478280	43.537677
3508.034075	1070981.214279	43.542682
3507.725846	1070833.738407	43.547687
3507.573300	1070678.640027	43.552692
3507.637383	1070518.407459	43.557697
3507.644785	1070377.018687	43.562701
3507.427947	1070220.572270	43.567706
3507.814912	1070067.866876	43.572711
3507.313856	1069928.376607	43.577716
3507.626013	1069777.501832	43.582721
3507.400891	1069641.131040	43.587725
3507.595126	1069470.752647	43.592730
3507.778544	1069331.807391	43.597735
3507.364554	1069187.284818	43.602740
3507.693901	1069024.753686	43.607745
3507.303130	1068888.872159	43.612749
3507.457260	1068730.206914	43.617754
3507.216396	1068582.370877	43.622759
3506.865301	1068450.798672	43.627764
3507.258959	1068286.312025	43.632769
3507.156254	1068162.961292	43.637773
3507.355526	1068023.211006	43.642778
3507.117483	1067880.259687	43.647783
3506.921939	1067737.009147	43.652788
3507.091988	1067579.077286	43.657793
3507.293252	1067450.371272	43.662797
3507.127225	1067305.565893	43.667802
3507.074726	1067164.681139	43.672807
3506.822185	1067021.132763	43.677812
3507.083947	1066889.710684	43.682817
3506.689775	1066759.643848	43.687821
3506.817001	1066621.793354	43.692826
3507.199875	1066476.587138	43.697831
3507.046003	1066340.507230	43.702836
3507.354363	1066194.728700	43.707841
3507.203745	1066069.414947	43.712845
3507.417783	1065915.468086	43.717850
3507.356560	1065770.797328	43.722855
3507.181483	1065638.070449	43.727860
3507.157762	1065478.763241	43.732865
3506.903626	1065346.138527	43.737869
3507.040399	1065201.997406	43.742874
3507.107174	1065071.044949	43.747879
3506.943042	1064932.526546	43.752884
3507.090564	1064792.702515	43.757889
3506.898084	1064658.222925	43.762893
3507.185290	1064521.929069	43.767898
3506.956989	1064367.819233	43.772903
3507.006176	1064242.911992	43.777908
3507.276996	1064109.208685	43.782913
3506.978956	1063961.353735	43.787917
3506.835352	1063814.624164	43.792922
3506.650782	1063691.378844	43.797927
3506.536152	1063561.575099	43.802932
3507.100313	1063418.664120	43.807937
3507.012008	1063289.523295	43.812941
3506.840057	1063159.911988	43.817946
3506.629791	1063024.914116	43.822951
3506.882918	1062888.585367	43.827956
3507.057884	1062753.613635	43.832961
3506.701914	1062619.303558	43.837965
3506.669699	1062476.466318	43.842970
3506.729834	1062352.958163	43.847975
3506.402633	1062214.301812	43.852980
3506.669335	1062073.426351	43.857985
3506.266876	1061948.733880	43.862989
3506.401754	1061824.142616	43.867994
3506.499471	1061696.666550	43.872999
3506.296172	1061567.793022	43.878004
3506.433712	1061438.186416	43.883009
3506.286426	1061324.509325	43.888013
3505.964702	1061206.333519	43.893018
3506.485389	1061077.618104	43.898023
3506.089153	1060955.597945	43.903028
3506.521267	1060830.935236	43.908033
3506.250970	1060716.591845	43.913037
3506.201162	1060577.848538	43.918042
3506.321065	1060453.710156	43.923047
3506.145593	1060340.884007	43.928052
3506.236595	1060207.885806	43.933057
3505.919453	1060081.788797	43.938061
3505.918784	1059969.311431	43.943066
3505.860214	1059847.114768	43.948071
3505.623296	1059737.464344	43.953076
3505.820334	1059609.923577	43.958081
3506.152507	1059509.805539	43.963085
3506.130306	1059388.748413	43.968090
3506.224517	1059276.722825	43.973095
3506.061358	1059143.933407	43.978100
3506.280528	1059010.981499	43.983105
3506.146656	1058914.589449	43.988109
3506.058773	1058778.600304	43.993114
3506.227592	1058659.807399	43.998119
3505.771267	1058547.087056	44.003124
3505.873908	1058433.405399	44.008129
3505.781701	1058324.569942	44.013133
3505.743664	1058200.695765	44.018138
3505.882429	1058089.505674	44.023143
3505.722939	1057976.339425	44.028148
3505.694891	1057858.910367	44.033153
3505.531251	1057759.227531	44.038157
3505.553535	1057643.037989	44.043162
3505.816472	1057529.118594	44.048167
3505.616486	1057427.605227	44.053172
3505.856803	1057300.870978	44.058177
3505.845774	1057197.877055	44.063181
3505.611447	1057097.712149	44.068186
3505.886956	1056987.633514	44.073191
3505.596403	1056862.132842	44.078196
3505.947781	1056739.125220	44.083201
3505.726687	1056631.337468	44.088205
3505.532856	1056521.808628	44.093210
3506.178778	1056407.706630	44.098215
3505.793380	1056299.361272	44.103220
3506.022265	1056179.155906	44.108225
3506.100968	1056064.465666	44.113229
3506.052191	1055945.746472	44.118234
3505.895507	1055826.367886	44.123239
3505.517810	1055720.419196	44.128244
3505.954127	1055600.167051	44.133249
3505.098419	1055502.677665	44.138253
3505.356010	1055390.642544	44.143258
3505.475568	1055285.663786	44.148263
3505.675166	1055181.055384	44.153268
3505.741083	1055058.924772	44.158273
3505.418488	1054961.048842	44.163277
3505.484396	1054847.106501	44.168282
3505.183670	1054747.488162	44.173287
3505.057851	1054641.188074	44.178292
3505.260600	1054548.809120	44.183297
3505.600327	1054443.778086	44.188301
3505.189935	1054334.723454	44.193306
3505.248179	1054223.565066	44.198311
3505.244031	1054129.767166	44.203316
3505.188186	1054026.335779	44.208321
3505.235346	1053917.583159	44.213325
3505.137634	1053812.515759	44.218330
3505.517643	1053714.791221	44.223335
3505.217768	1053616.502054	44.228340
3505.252508	1053504.658183	44.233345
3505.407466	1053405.229797	44.238349
3505.069372	1053310.894494	44.243354
3505.080141	1053201.362428	44.248359
3505.295781	1053100.568704	44.253364
3505.392803	1053004.228091	44.258369
3504.908040	1052897.664273	44.263373
3504.904802	1052800.854506	44.268378
3505.110713	1052711.529914	44.273383
3505.086792	1052615.973866	44.278388
3504.954435	1052518.601845	44.283393
3504.500777	1052417.230871	44.288397
3504.694497	1052331.663003	44.293402
3504.755812	1052235.797038	44.298407
3504.804225	1052134.627492	44.303412
3504.995967	1052049.441330	44.308417
3504.931818	1051961.209915	44.313421
3504.757156	1051861.229387	44.318426
3505.025781	1051774.001037	44.323431
3504.460634	1051686.233517	44.328436
3504.594692	1051584.461123	44.333441
3504.595083	1051503.734617	44.338445
3504.998941	1051409.437520	44.343450
3504.978686	1051323.696392	44.348455
3504.583767	1051221.618635	44.353460
3504.578652	1051126.998267	44.358465
3504.630279	1051045.484991	44.363469
3504.692312	1050960.303410	44.368474
3504.722184	1050869.241801	44.373479
3504.760474	1050772.293192	44.378484
3504.703409	1050685.101305	44.383489
3504.819767	1050603.281463	44.388493
3504.884603	1050515.488042	44.393498
3504.723468	1050409.401691	44.398503
3504.716892	1050320.266390	44.403508
3505.044847	1050227.505150	44.408513
3504.818757	1050129.913528	44.413517
3504.758589	1050042.519076	44.418522
3504.977976	1049939.641145	44.423527
3504.878276	1049856.881091	44.428532
3504.925332	1049763.000605	44.433537
3504.835778	1049674.350953	44.438541
3504.555297	1049574.153516	44.443546
3504.461634	1049478.651188	44.448551
3504.213352	1049409.127130	44.453556
3504.802373	1049312.544650	44.458561
3504.859211	1049224.442596	44.463565
3504.617141	1049124.906108	44.468570
3504.397618	1049044.179911	44.473575
3504.538604	1048964.937039	44.478580
3504.531055	1048880.217343	44.483585
3504.606916	1048804.167196	44.488589
3504.325474	1048707.717533	44.493594
3504.402696	1048619.795488	44.498599
3504.550999	1048540.255836	44.503604
3504.185691	1048448.254454	44.508609
3504.446393	1048369.755357	44.513613
3504.531034	1048292.828213	44.518618
3504.544370	1048194.776990	44.523623
3504.389760	1048114.123035	44.528628
3504.379534	1048016.458564	44.533633
3504.466862	1047948.211993	44.538637
3504.341049	1047867.742724	44.543642
3504.806424	1047776.365450	44.548647
3504.371530	1047687.451299	44.553652
3504.519214	1047599.694479	44.558657
3504.450061	1047527.221774	44.563661
3504.287961	1047443.856793	44.568666
3504.456042	1047353.969302	44.573671
3504.018507	1047267.751415	44.578676
3504.085993	1047190.329168	44.583681
3504.037614	1047118.426830	44.588685
3504.135503	1047027.966462	44.593690
3504.334569	1046952.932382	44.598695
3503.958912	1046880.212106	44.603700
3504.090003	1046800.264182	44.608705
3504.313383	1046725.995266	44.613709
3504.140210	1046641.751248	44.618714
3504.036251	1046565.120763	44.623719
3503.690048	1046489.301401	44.628724
3503.861424	1046416.002251	44.633729
3503.790232	1046351.527052	44.638733
3504.139789	1046266.901624	44.643738
3504.275392	1046192.543478	44.648743
3503.986607	1046120.957409	44.653748
3504.388142	1046032.458160	44.658753
3504.493783	1045963.604859	44.663757
3503.745300	1045886.491870	44.668762
3504.430621	1045812.713913	44.673767
3504.038880	1045738.533077	44.678772
3504.264084	1045654.304976	44.683777
3504.538413	1045574.122673	44.688781
3504.415456	1045498.156420	44.693786
3504.312665	1045391.964251	44.698791
3504.020787	1045321.140791	44.703796
3504.299361	1045240.083955	44.708801
3504.232829	1045164.296946	44.713805
3504.065655	1045088.622037	44.718810
3504.226761	1045014.533570	44.723815
3503.956515	1044927.286063	44.728820
3503.885650	1044853.813030	44.733825
3503.980320	1044779.346105	44.738829
3503.805096	1044705.405466	44.743834
3504.062575	1044633.420502	44.748839
3504.408137	1044567.600523	44.753844
3504.147608	1044480.344380	44.758849
3503.849826	1044399.177040	44.763853
3503.626147	1044324.756443	44.768858
3503.958554	1044259.900714	44.773863
3503.956781	1044184.089639	44.778868
3503.999773	1044104.213915	44.783873
3504.239924	1044042.461310	44.788877
3504.034923	1043972.765244	44.793882
3504.074967	1043881.007505	44.798887
3503.620261	1043816.565977	44.803892
3504.300901	1043741.698867	44.808897
3504.121337	1043674.988956	44.813901
3504.061411	1043593.770648	44.818906
3503.909238	1043512.373168	44.823911
3504.137732	1043443.758107	44.828916
3504.160779	1043379.715756	44.833921
3503.883822	1043297.080002	44.838925
3503.481159	1043220.162683	44.843930
3503.918579	1043134.509071	44.848935
3503.417310	1043083.396648	44.853940
3503.615188	1043009.178747	44.858945
3503.501190	1042952.012359	44.863949
3503.642948	1042883.694451	44.868954
3503.402219	1042818.433286	44.873959
3503.176653	1042752.106247	44.878964
3503.681195	1042685.078554	44.883969
3503.647077	1042625.577201	44.888973
3503.627607	1042558.924101	44.893978
3503.928720	1042484.585581	44.898983
3503.682608	1042424.537355	44.903988
3503.601735	1042347.265110	44.908993
3503.849241	1042279.598607	44.913997
3503.250654	1042210.814700	44.919002
3503.693737	1042144.370269	44.924007
3503.393475	1042082.008583	44.929012
3503.613262	1042024.294601	44.934017
3503.539348	1041964.599489	44.939021
3503.278535	1041901.649591	44.944026
3503.322746	1041824.832548	44.949031
3503.297433	1041777.494363	44.954036
3503.492025	1041710.216109	44.959041
3503.209160	1041647.653437	44.964045
3503.063054	1041590.091825	44.969050
3503.576221	1041536.479154	44.974055
3503.590070	1041470.677096	44.979060
3503.342345	1041393.129179	44.984065
3503.266356	1041332.654619	44.989069
3503.391628	1041287.026708	44.994074
3503.404044	1041209.336753	44.999079
3503.345219	1041149.340506	45.004084
3503.421846	1041073.763908	45.009089
3503.729015	1041027.524129	45.014093
3503.606870	1040965.700344	45.019098
3503.944162	1040897.035897	45.024103
3503.511862	1040825.791595	45.029108
3503.147814	1040759.366909	45.034113
3503.360686	1040710.820776	45.039117
3503.483948	1040651.562253	45.044122
3503.337554	1040570.893768	45.049127
3503.200571	1040529.265012	45.054132
3503.109834	1040465.304416	45.059137
3503.516733	1040398.748440	45.064141
3503.449242	1040339.131436	45.069146
3503.431965	1040267.521686	45.074151
3503.502103	1040218.124964	45.079156
3503.240404	1040147.037141	45.084161
3503.363277	1040087.386082	45.089165
3503.582279	1040040.669383	45.094170
3503.496948	1039970.806679	45.099175
3503.261406	1039918.944767	45.104180
3503.395609	1039850.300840	45.109185
3503.601655	1039794.112379	45.114189
3503.512092	1039730.336432	45.119194
3503.796427	1039657.219343	45.124199
3503.267349	1039604.436293	45.129204
3503.016250	1039539.524895	45.134209
3503.385539	1039479.923390	45.139213
3503.475644	1039410.411377	45.144218
3503.172365	1039357.202151	45.149223
3502.946406	1039307.169482	45.154228
3503.399975	1039242.815183	45.159233
3503.531213	1039181.606440	45.164237
3503.372327	1039124.118034	45.169242
3503.677125	1039079.505735	45.174247
3503.323742	1039013.928390	45.179252
3503.202818	1038933.908600	45.184257
3503.253910	1038876.093043	45.189261
3503.319180	1038826.878097	45.194266
3503.525888	1038753.665246	45.199271
3503.308170	1038700.628979	45.204276
3503.238080	1038647.567891	45.209281
3503.340729	1038586.840671	45.214285
3503.182137	1038519.098592	45.219290
3503.296207	1038456.434581	45.224295
3503.021449	1038403.501547	45.229300
3503.341329	1038337.998690	45.234305
3503.315867	1038277.482548	45.239309
3502.940551	1038230.751854	45.244314
3503.222113	1038173.277750	45.249319
3502.933359	1038118.990786	45.254324
3503.092610	1038072.557443	45.259329
3502.973233	1038035.644521	45.264333
3503.089952	1037971.911105	45.269338
3503.561016	1037899.030205	45.274343
3503.012985	1037846.523614	45.279348
3502.742772	1037787.686115	45.284353
3502.964036	1037732.634568	45.289357
3502.719101	1037674.081766	45.294362
3503.045498	1037619.301851	45.299367
3502.864273	1037592.065160	45.304372
3502.871118	1037530.665356	45.309377
3502.932533	1037485.983681	45.314381
3503.077881	1037423.012801	45.319386
3503.060057	1037372.831742	45.324391
3502.908071	1037324.509534	45.329396
3503.032760	1037276.818209	45.334401
3503.139432	1037215.881970	45.339405
3502.992834	1037173.456076	45.344410
3502.934474	1037109.161428	45.349415
3503.041518	1037057.796575	45.354420
3503.024247	1037006.451724	45.359425
3503.057491	1036951.810225	45.364429
3502.922053	1036902.611312	45.369434
3503.039257	1036836.834065	45.374439
3503.035803	1036788.095919	45.379444
3502.587454	1036742.815304	45.384449
3502.945756	1036692.662868	45.389453
3502.872986	1036653.798974	45.394458
3503.239787	1036578.016756	45.399463
3503.177757	1036535.958903	45.404468
3502.853039	1036477.309931	45.409473
3503.001292	1036437.731157	45.414477
3503.034546	1036388.306491	45.419482
3503.056167	1036322.829048	45.424487
3502.967050	1036282.901419	45.429492
3502.691324	1036221.630424	45.434497
3503.139334	1036165.365466	45.439501
3503.028183	1036114.027843	45.444506
3503.414910	1036075.084229	45.449511
3503.018082	1036027.274662	45.454516
3503.032930	1035964.212057	45.459521
3502.984860	1035907.542607	45.464525
3502.824843	1035860.272918	45.469530
3502.780515	1035811.339511	45.474535
3502.756092	1035762.982728	45.479540
3503.029588	1035713.802673	45.484545
3503.245889	1035655.152650	45.489549
3503.269344	1035602.917627	45.494554
3503.104697	1035545.006261	45.499559
3502.984824	1035488.247643	45.504564
3503.141667	1035434.344710	45.509569
3503.240817	1035384.803556	45.514573
3502.902337	1035335.237309	45.519578
3503.153136	1035272.708390	45.524583
3502.919326	1035224.768343	45.529588
3503.158950	1035176.556443	45.534593
3503.671869	1035116.110710	45.539597
3503.135218	1035054.869842	45.544602
3502.937434	1035004.987277	45.549607
3502.946869	1034948.492065	45.554612
3503.158352	1034895.832497	45.559617
3502.852683	1034848.868419	45.564621
3502.784184	1034794.706198	45.569626
3503.090787	1034737.869690	45.574631
3503.191996	1034688.805708	45.579636
3502.982698	1034632.827025	45.584641
3502.852641	1034584.961120	45.589645
3502.752158	1034544.926153	45.594650
3502.624050	1034495.414520	45.599655
3503.116175	1034445.219823	45.604660
3502.824585	1034379.867865	45.609665
3502.825199	1034333.139229	45.614669
3502.656036	1034289.921087	45.619674
3502.910269	1034243.440171	45.624679
3502.917265	1034198.160582	45.629684
3502.894992	1034157.335953	45.634689
3502.771542	1034102.402049	45.639693
3502.677211	1034055.009461	45.644698
3502.674079	1034009.052739	45.649703
3503.220171	1033959.812315	45.654708
3502.663802	1033914.719962	45.659713
3502.924560	1033859.333365	45.664717
3502.680149	1033826.476827	45.669722
3502.972284	1033753.958201	45.674727
3502.432956	1033705.281328	45.679732
3502.904497	1033669.596723	45.684737
3503.040819	1033610.164284	45.689741
3502.392324	1033570.599610	45.694746
3502.667809	1033525.270333	45.699751
3502.624693	1033475.155066	45.704756
3502.772688	1033436.619400	45.709761
3502.846792	1033379.904108	45.714765
3502.770750	1033337.824403	45.719770
3502.918143	1033285.160178	45.724775
3502.613991	1033242.439966	45.729780
3502.704557	1033187.268258	45.734785
3502.537958	1033154.878775	45.739789
3502.367372	1033113.490320	45.744794
3502.356566	1033070.333401	45.749799
3502.447983	1033030.546251	45.754804
3502.282756	1033004.252152	45.759809
3502.599817	1032947.589217	45.764813
3502.118756	1032892.702283	45.769818
3502.306675	1032781.575987	45.774823
3502.615035	1032628.233174	45.779828
3502.103291	1032412.211083	45.784833
3502.527834	1032123.050673	45.789837
3502.386823	1031787.702401	45.794842
3502.272472	1031373.052213	45.799847
3502.286826	1030907.914044	45.804852
3502.442146	1030369.134323	45.809857
3502.369988	1029750.942841	45.814861
3501.854469	1029101.864751	45.819866
3502.127726	1028359.217998	45.824871
3502.124323	1027559.368306	45.829876
3501.710678	1026685.649868	45.834881
3501.721937	1025747.192558	45.839885
3501.233966	1024743.825380	45.844890
3501.095278	1023653.951752	45.849895
3500.948065	1022492.317025	45.854900
3500.710136	1021267.714853	45.859905
3500.969819	1019947.319584	45.864909
3500.526177	1018572.107267	45.869914
3500.751044	1017098.820837	45.874919
3500.437637	1015559.324971	45.879924
3500.073121	1013927.268309	45.884929
3499.849126	1012209.823909	45.889933
3499.190041	1010430.716215	45.894938
3499.201798	1008557.826001	45.899943
3499.018056	1006611.718119	45.904948
3498.767180	1004575.761998	45.909953
3498.234576	1002456.999466	45.914957
3497.941701	1000272.870263	45.919962
3497.643359	997993.738429	45.924967
3497.487392	995627.064615	45.929972
3496.721236	993178.029865	45.934977
3496.239440	990645.699201	45.939981
3495.929573	988045.783992	45.944986
3495.277988	985349.391112	45.949991
3494.954930	982590.058327	45.954996
3494.777624	979736.759884	45.960001
3494.586723	976799.157516	45.965005
3493.797996	973776.242372	45.970010
3493.373442	970669.387038	45.975015
3493.123703	967488.279262	45.980020
3492.270136	964231.654038	45.985025
3492.462620	960870.594279	45.990029
3491.437572	957430.007434	45.995034
3490.929369	953936.297482	46.000039
3490.361947	950433.331265	46.005044
3489.736134	946849.260355	46.010049
3489.216176	943177.102564	46.015053
3488.212257	939444.695698	46.020058
3487.862541	935618.345099	46.025063
3487.093699	931710.338584	46.030068
3486.139992	927723.652105	46.035073
3485.752498	923657.337179	46.040077
3484.860747	919512.571197	46.045082
3484.128992	915285.624229	46.050087
3483.406505	910978.384376	46.055092
3482.366133	906598.949521	46.060097
3482.082731	902139.375395	46.065101
3481.091658	897591.338159	46.070106
3480.220613	892954.039767	46.075111
3479.271458	888265.278480	46.080116
3478.395403	883484.834358	46.085121
3477.724936	878615.214933	46.090125
3477.057686	873672.868341	46.095130
3475.658911	868631.652209	46.100135
3474.996031	863528.059299	46.105140
3474.058525	858345.024317	46.110145
3473.178835	853058.192811	46.115149
3472.175219	847691.354824	46.120154
3471.239727	842245.302840	46.125159
3470.205746	836736.268204	46.130164
3469.120543	831140.347488	46.135169
3468.040634	825449.347939	46.140173
3466.981625	819684.713352	46.145178
3466.027380	813829.796972	46.150183
3464.693185	807908.826443	46.155188
3463.504665	801894.086426	46.160193
3462.766152	795806.274736	46.165197
3461.290229	789645.618623	46.170202
3460.063671	783359.203584	46.175207
3458.917881	777028.691715	46.180212
3457.493279	770615.227556	46.185217
3456.598282	764129.546228	46.190221
3455.167093	757552.767045	46.195226
3454.058181	750899.771390	46.200231
3452.888364	744153.458159	46.205236
3451.529361	737346.221890	46.210241
3450.107276	730415.370747	46.215245
3448.320785	723433.769564	46.220250
3447.271660	716347.871151	46.225255
3446.072711	709203.504475	46.230260
3444.453887	701970.359142	46.235265
3443.343400	694655.934768	46.240269
3441.611263	687278.355901	46.245274
3440.407061	679790.760707	46.250279
3438.886487	672241.813288	46.255284
3436.854635	664616.402600	46.260289
3435.821755	656908.332880	46.265293
3434.353024	649114.979040	46.270298
3432.733629	641239.131994	46.275303
3430.961769	633296.610369	46.280308
3429.160828	625276.112019	46.285313
3427.488279	617174.071775	46.290317
3425.724070	609002.385210	46.295322
3424.183219	600757.686828	46.300327
3422.419138	592444.269391	46.305332
3420.537337	584043.626136	46.310337
3419.041854	575565.214811	46.315341
3417.274849	567043.337050	46.320346
3415.054747	558417.043779	46.325351
3413.124218	549724.796624	46.330356
3411.186882	540952.267536	46.335361
3409.384661	532117.078464	46.340365
3406.942283	523224.173303	46.345370
3405.419358	514245.028940	46.350375
3403.402496	505210.812680	46.355380
3401.074049	496109.908624	46.360385
3399.263899	486930.828409	46.365389
3396.923801	477677.012303	46.370394
3394.780744	468369.508047	46.375399
3392.631628	458995.703429	46.380404
3390.279272	449555.595783	46.385409
3388.092099	440051.024508	46.390413
3385.841855	430483.075115	46.395418
3383.566602	420859.323045	46.400423
3381.019924	411163.434129	46.405428
3378.555024	401400.986403	46.410433
3376.026066	391592.396919	46.415437
3373.323485	381732.179144	46.420442
3370.796926	371804.471374	46.425447
3368.197182	361849.384149	46.430452
3365.471137	351827.764467	46.435457
3363.076811	341757.678781	46.440461
3360.032025	331638.084316	46.445466
3357.120130	321454.441225	46.450471
3354.385463	311245.491306	46.455476
3351.147128	300990.386304	46.460481
3348.114542	290689.283111	46.465485
3345.035169	280360.076291	46.470490
3341.616446	269975.954812	46.475495
3338.516801	259584.805287	46.480500
3335.116104	249144.650759	46.485505
3331.823783	238667.851803	46.490509
3328.194823	228155.658760	46.495514
3324.866493	217563.825896	46.500519
3321.083083	207019.694078	46.505524
3317.147268	196467.429720	46.510529
3313.672257	185893.505561	46.515533
3309.309581	175301.982723	46.520538
3305.265177	164694.670281	46.525543
3301.291830	154098.860587	46.530548
3296.727583	143508.692819	46.535553
3292.330985	132910.923490	46.540557
3287.507658	122310.882633	46.545562
3282.501541	111732.437792	46.550567
3277.558235	101184.636532	46.555572
3271.843391	90665.906987	46.560577
3266.469125	80159.960080	46.565581
3260.287750	69709.856362	46.570586
3253.261292	59317.053409	46.575591
3246.374439	49008.297785	46.580596
3237.320193	38818.555153	46.585601
3213.718371	29117.118237	46.590605
3157.675487	20571.060885	46.595610
3097.897018	12774.446306	46.600615
3039.947542	5841.196627	46.605620
2949.649724	887.057687	46.610625
2753.166843	396.514074	46.615629
2634.845298	400.967046	46.620634
2619.155708	392.107767	46.625639
2672.003692	381.909289	46.630644
2750.575365	367.980258	46.635649
2820.313602	346.156553	46.640653
2864.028634	356.379993	46.645658
2881.606471	359.011645	46.650663
2880.104395	369.156098	46.655668
2870.026442	353.204879	46.660673
2858.191570	349.384597	46.665677
2848.381170	343.557047	46.670682
2842.650090	343.187040	46.675687
2839.383036	347.710552	46.680692
2837.225879	344.788851	46.685697
2836.312458	330.169115	46.690701
2834.649018	342.580291	46.695706
2833.312433	328.723295	46.700711
2831.075693	326.814226	46.705716
2827.933989	344.026229	46.710721
2824.433186	330.618074	46.715725
2821.471350	333.304274	46.720730
2818.279030	329.375161	46.725735
2815.743413	325.799308	46.730740
2811.994059	326.122941	46.735745
2809.084865	312.332550	46.740749
2805.720285	334.953422	46.745754
2802.623234	325.884501	46.750759
2799.913166	316.143068	46.755764
2796.651495	318.316355	46.760769
2793.191253	312.175118	46.765773
2790.164961	316.983433	46.770778
2786.522310	323.437169	46.775783
2783.067987	319.804623	46.780788
2779.768413	315.557381	46.785793
2777.016342	304.203715	46.790797
2773.811053	314.064422	46.795802
2770.207173	308.504593	46.800807
2766.907855	296.573837	46.805812
2763.578448	309.543099	46.810817
2761.100881	301.238989	46.815821
2757.267156	310.089754	46.820826
2753.361673	315.948910	46.825831
2750.101030	307.698826	46.830836
2746.879093	298.343220	46.835841
2743.713584	303.063312	46.840845
2740.166979	306.200130	46.845850
2736.799289	295.428845	46.850855
2733.822108	295.173255	46.855860
2730.125446	310.588131	46.860865
2726.667964	297.052362	46.865869
2722.740584	296.461331	46.870874
2719.690591	303.484102	46.875879
2716.560241	293.585891	46.880884
2713.205747	301.422577	46.885889
2709.697093	302.112156	46.890893
2706.006636	288.544376	46.895898
2702.601598	289.190138	46.900903
2699.594509	300.491635	46.905908
2696.165148	293.052256	46.910913
2692.626827	292.597468	46.915917
2688.548498	292.834319	46.920922
2685.418916	289.197813	46.925927
2682.386941	287.341576	46.930932
2678.702760	297.676878	46.935937
2675.634493	281.856389	46.940941
2671.621627	289.397533	46.945946
2668.003449	290.408660	46.950951
2665.367875	277.924183	46.955956
2661.601977	301.116429	46.960961
2658.086758	289.825616	46.965965
2655.033084	287.761544	46.970970
2651.009555	293.134283	46.975975
2647.134699	280.364016	46.980980
2644.056342	277.195207	46.985985
2641.127500	287.315801	46.990989
2637.587844	286.370536	46.995994
2633.407308	278.119284	47.000999
2629.987656	282.264605	47.006004
2626.139864	274.065934	47.011009
2623.639924	270.409008	47.016013
2620.261427	284.722012	47.021018
2616.607272	283.083920	47.026023
2613.550608	277.393113	47.031028
2609.764756	274.622840	47.036033
2606.158111	275.179945	47.041037
2602.704202	265.069378	47.046042
2599.446860	268.284933	47.051047
2596.390606	281.526562	47.056052
2592.308865	277.477944	47.061057
2588.831441	271.836502	47.066061
2585.368646	276.558405	47.071066
2581.571603	281.294088	47.076071
2578.097845	265.935755	47.081076
2574.588998	273.920461	47.086081
2571.835612	271.070631	47.091085
2568.033663	263.217339	47.096090
2564.336734	258.994597	47.101095
2561.122107	261.963385	47.106100
2557.425799	275.973143	47.111105
2554.503991	261.072847	47.116109
2550.611444	260.251520	47.121114
2547.381373	270.271741	47.126119
2543.773833	268.381724	47.131124
2539.899721	273.197219	47.136129
2536.294422	258.886056	47.141133
2533.018549	278.199776	47.146138
2529.709200	265.315530	47.151143
2526.195337	259.311450	47.156148
2522.833221	268.519402	47.161153
2519.550602	266.388172	47.166157
2516.277056	268.752650	47.171162
2512.017748	273.012402	47.176167
2508.689031	260.446083	47.181172
2504.849589	267.468761	47.186177
2501.598107	267.989348	47.191181
2498.386332	264.110864	47.196186
2495.228984	263.676713	47.201191
2491.927496	268.733039	47.206196
2488.370273	265.220519	47.211201
2484.578313	259.273272	47.216205
2480.756588	264.584390	47.221210
2477.460269	263.243810	47.226215
2474.083572	260.114311	47.231220
2470.491965	270.552697	47.236225
2467.257904	257.320642	47.241229
2463.261414	256.501112	47.246234
2460.234956	261.046629	47.251239
2456.624269	254.362625	47.256244
2452.805555	252.723539	47.261249
2449.540443	248.024071	47.266253
2445.668557	252.705160	47.271258
2442.576604	251.745651	47.276263
2439.069497	258.857786	47.281268
2435.676981	264.529572	47.286273
2432.442177	250.572337	47.291277
2428.750645	255.301435	47.296282
2425.198243	260.622917	47.301287
2421.526393	248.381592	47.306292
2417.868838	254.692684	47.311297
2414.802385	261.231671	47.316301
2411.515818	256.981885	47.321306
2407.373400	253.767866	47.326311
2404.409122	247.676478	47.331316
2400.870399	264.637569	47.336321
2397.345172	249.342707	47.341325
2393.636778	251.335480	47.346330
2390.130714	252.329034	47.351335
2386.694732	243.137302	47.356340
2383.121477	247.637463	47.361345
2379.720901	259.509527	47.366349
2376.182655	254.660486	47.371354
2372.774487	252.226533	47.376359
2369.301446	241.513217	47.381364
2365.809994	239.192549	47.386369
2362.414338	242.301368	47.391373
2358.795007	251.872717	47.396378
2355.218081	242.488978	47.401383
2351.604522	244.414335	47.406388
2347.882924	251.741432	47.411393
2345.218371	243.919227	47.416397
2341.548648	245.556499	47.421402
2338.011089	233.787955	47.426407
2334.434676	237.101711	47.431412
2330.428080	254.394213	47.436417
2327.473603	243.465859	47.441421
2324.175891	238.815635	47.446426
2320.608504	246.015296	47.451431
2316.890031	235.445194	47.456436
2313.028703	240.717331	47.461441
2309.790236	242.628004	47.466445
2306.137858	240.568414	47.471450
2302.586262	234.885599	47.476455
2299.844245	231.738236	47.481460
2296.134868	240.798612	47.486465
2292.539888	240.092510	47.491469
2288.629617	244.258795	47.496474
2284.980957	246.984261	47.501479
2281.684010	234.613523	47.506484
2278.273310	236.261280	47.511489
2275.246547	235.480611	47.516493
2271.661458	233.832687	47.521498
2267.722106	231.802592	47.526503
2264.649102	233.751600	47.531508
2260.814635	241.068733	47.536513
2257.488258	219.215722	47.541517
2254.179008	239.090006	47.546522
2250.423979	238.552092	47.551527
2246.827065	229.963344	47.556532
2243.514236	233.689263	47.561537
2239.846514	223.566148	47.566541
2236.613136	234.732102	47.571546
2232.823747	234.668190	47.576551
2229.780232	229.869243	47.581556
2225.765579	228.182783	47.586561
2222.565172	227.796103	47.591565
2218.867968	228.894957	47.596570
2215.392120	237.351936	47.601575
2211.906907	226.107982	47.606580
2208.311829	233.903106	47.611585
2205.395800	235.692663	47.616589
2201.360424	224.523576	47.621594
2197.661141	225.118745	47.626599
2194.677503	218.742679	47.631604
2191.009442	236.557995	47.636609
2187.379229	227.235045	47.641613
2184.016217	221.366303	47.646618
2180.389597	230.432208	47.651623
2176.953164	223.211154	47.656628
2173.118921	232.661936	47.661633
2169.667001	236.569074	47.666637
2166.650823	240.045427	47.671642
2162.821822	221.848046	47.676647
2159.871575	220.695299	47.681652
2155.983506	226.395844	47.686657
2152.457538	227.293441	47.691661
2149.064427	228.747452	47.696666
2145.219689	230.535031	47.701671
2142.054361	233.202935	47.706676
2138.660489	220.484038	47.711681
2135.132504	222.667277	47.716685
2131.401789	227.695478	47.721690
2127.744722	236.916487	47.726695
2124.662357	227.732485	47.731700
2120.914826	222.685083	47.736705
2117.533620	221.326314	47.741709
2113.884044	220.012801	47.746714
2110.327415	228.494584	47.751719
2107.121048	226.826794	47.756724
2103.374950	226.571417	47.761729
2100.039547	231.428567	47.766733
2096.423559	228.550350	47.771738
2092.779041	223.677266	47.776743
2089.519755	213.529495	47.781748
2085.756888	229.554267	47.786753
2082.533332	221.415961	47.791757
2079.161957	224.574264	47.796762
2075.536557	225.249549	47.801767
2072.105753	226.904659	47.806772
2068.714343	213.521641	47.811777
2065.098161	218.651634	47.816781
2061.483104	214.096811	47.821786
2057.724628	227.841207	47.826791
2054.536039	219.329653	47.831796
2051.026112	214.433505	47.836801
2047.526556	218.663757	47.841805
2044.219614	223.631759	47.846810
2040.195540	228.280126	47.851815
2037.146693	216.675235	47.856820
2033.378678	223.140943	47.861825
2030.000330	222.286866	47.866829
2026.086589	220.136366	47.871834
2022.703173	225.099826	47.876839
2019.641000	206.919712	47.881844
2016.285915	221.518235	47.886849
2012.811016	218.603471	47.891853
2009.228872	205.938906	47.896858
2005.545497	220.053515	47.901863
2002.184383	208.119743	47.906868
1998.732619	206.927168	47.911873
1994.843897	206.059042	47.916877
1991.272559	210.242851	47.921882
1987.832174	204.281715	47.926887
1984.433078	200.718622	47.931892
1981.148006	204.397345	47.936897
1977.565562	206.653764	47.941901
1973.832733	204.918885	47.946906
1970.210089	211.441533	47.951911
1966.894711	205.617537	47.956916
1963.652831	208.412185	47.961921
1960.316238	211.999281	47.966925
1956.450845	209.896587	47.971930
1952.787718	213.542587	47.976935
1949.837660	204.786145	47.981940
1945.956232	215.472280	47.986945
1942.367652	213.652846	47.991949
1939.228795	197.541741	47.996954
1935.232832	210.578419	48.001959
1931.798822	200.090101	48.006964
1928.299537	205.901918	48.011969
1925.168351	211.174723	48.016973
1921.806835	209.155452	48.021978
1917.759576	202.820627	48.026983
1914.388889	193.308639	48.031988
1910.875651	200.744279	48.036993
1907.624743	204.484186	48.041997
1903.965235	198.275217	48.047002
1900.526047	202.452850	48.052007
1896.794779	204.281323	48.057012
1892.662264	198.860131	48.062017
1889.804379	195.192111	48.067021
1887.112708	197.122944	48.072026
1883.597414	204.157700	48.077031
1879.784463	195.628308	48.082036
1875.803521	202.955060	48.087041
1872.402972	199.039074	48.092045
1868.811700	198.758276	48.097050
1865.077705	200.015007	48.102055
1861.972066	204.913066	48.107060
1858.608766	203.484086	48.112065
1854.871331	197.626196	48.117069
1851.443912	191.939829	48.122074
1847.818122	207.991372	48.127079
1844.780641	191.891426	48.132084
1840.681723	190.755979	48.137089
1837.143517	192.334498	48.142093
1834.191678	190.674073	48.147098
1830.445804	203.987989	48.152103
1827.102487	197.693549	48.157108
1823.357834	195.959518	48.162113
1819.900741	190.184736	48.167117
1816.545322	196.723930	48.172122
1812.534139	203.900515	48.177127
1809.400475	197.207058	48.182132
1805.601986	201.898918	48.187137
1802.079009	188.619184	48.192141
1798.948902	195.680886	48.197146
1795.206497	202.925305	48.202151
1792.410884	197.657503	48.207156
1788.381752	195.736909	48.212161
1784.883888	198.074764	48.217165
1781.689569	195.067755	48.222170
1777.911527	201.661603	48.227175
1774.337791	184.076817	48.232180
1771.219503	197.323307	48.237185
1767.451040	196.364924	48.242189
1764.263206	186.821376	48.247194
1760.257913	199.359173	48.252199
1756.936112	208.767592	48.257204
1753.213313	200.222118	48.262209
1749.780845	196.805336	48.267213
1746.378809	192.442848	48.272218
1742.899573	196.670071	48.277223
1739.676198	186.511162	48.282228
1735.627187	196.931425	48.287233
1732.048711	198.449454	48.292237
1728.730180	195.291797	48.297242
1725.037855	201.381105	48.302247
1722.056842	185.365645	48.307252
1718.204247	199.894500	48.312257
1715.007105	197.064385	48.317261
1711.599359	185.045762	48.322266
1708.077187	198.264008	48.327271
1704.738689	188.783038	48.332276
1700.683016	188.514236	48.337281
1697.264327	189.961323	48.342285
1693.717540	191.999682	48.347290
1689.688642	196.923376	48.352295
1687.022323	192.274468	48.357300
1683.708048	191.438991	48.362305
1679.821448	189.840929	48.367309
1676.486204	183.050780	48.372314
1673.095019	189.825206	48.377319
1669.383992	184.053540	48.382324
1665.569730	190.411111	48.387329
1662.508768	185.428470	48.392333
1659.030557	182.230509	48.397338
1655.386779	187.588684	48.402343
1651.788997	189.399887	48.407348
1648.206249	194.539340	48.412353
1644.435593	187.689547	48.417357
1641.403378	188.999189	48.422362
1637.825535	190.966241	48.427367
1634.449826	188.950344	48.432372
1630.940074	185.748624	48.437377
1627.210817	182.881168	48.442381
1623.724681	186.499196	48.447386
1620.295345	185.586645	48.452391
1616.910290	175.455874	48.457396
1613.408026	184.550000	48.462401
1609.780595	184.343767	48.467405
1606.100850	180.310721	48.472410
1602.477356	192.588659	48.477415
1599.314988	185.537095	48.482420
1596.074966	185.852166	48.487425
1592.185348	178.102665	48.492429
1589.013802	179.745003	48.497434
1585.057348	185.705604	48.502439
1581.565613	180.175124	48.507444
1578.130786	183.744256	48.512449
1574.622745	186.024792	48.517453
1571.227626	180.111965	48.522458
1567.549926	177.629377	48.527463
1564.202909	187.215452	48.532468
1560.685444	184.524600	48.537473
1557.113269	185.767509	48.542477
1553.956048	174.895958	48.547482
1550.053941	186.991600	48.552487
1546.999331	179.920902	48.557492
1543.730727	184.515572	48.562497
1539.951433	187.038596	48.567501
1536.443910	180.276363	48.572506
1532.695200	173.453212	48.577511
1529.123869	183.280139	48.582516
1525.384060	190.329597	48.587521
1521.821080	184.858754	48.592525
1518.888761	184.731514	48.597530
1515.164258	186.202123	48.602535
1511.947877	177.433243	48.607540
1508.356507	171.845948	48.612545
1504.962126	183.540538	48.617549
1501.357360	186.509806	48.622554
1497.413703	176.330117	48.627559
1494.252936	167.770301	48.632564
1490.654992	181.742513	48.637569
1487.215659	173.783709	48.642573
1483.712213	172.585517	48.647578
1479.874430	172.524069	48.652583
1476.632727	176.555144	48.657588
1473.421281	174.082476	48.662593
1469.596872	174.275331	48.667597
1466.093819	173.522810	48.672602
1462.586973	172.092166	48.677607
1459.223235	167.907115	48.682612
1455.573328	171.762777	48.687617
1452.078424	182.687393	48.692621
1448.826668	170.910160	48.697626
1444.789562	178.701575	48.702631
1441.537032	170.633635	48.707636
1438.517869	168.352014	48.712641
1434.720890	172.462813	48.717645
1431.345080	169.143006	48.722650
1427.473858	179.163505	48.727655
1424.481653	175.512833	48.732660
1420.827833	175.600707	48.737665
1417.393192	170.037913	48.742669
1413.778790	173.585848	48.747674
1409.878445	170.572233	48.752679
1406.466149	165.912601	48.757684
1403.233751	174.553237	48.762689
1399.666849	184.065860	48.767693
1396.241752	174.844529	48.772698
1392.388245	176.401606	48.777703
1389.000460	176.754675	48.782708
1385.075137	176.024833	48.787713
1382.138837	169.613844	48.792717
1378.792266	173.106146	48.797722
1375.559783	171.185227	48.802727
1371.440482	174.768769	48.807732
1368.409605	171.832165	48.812737
1364.330737	174.894252	48.817741
1361.000542	174.773654	48.822746
1357.462344	182.574024	48.827751
1353.861433	167.619066	48.832756
1350.322744	173.917583	48.837761
1347.062081	177.772881	48.842765
1343.769774	172.077224	48.847770
1339.972594	168.715732	48.852775
1336.447217	170.599389	48.857780
1333.116706	173.230166	48.862785
1329.619112	170.267520	48.867789
1326.706962	156.421643	48.872794
1322.401948	174.342695	48.877799
1319.109932	170.982577	48.882804
1315.271410	172.585069	48.887809
1311.666446	173.386109	48.892813
1308.729291	164.610031	48.897818
1305.370152	174.271498	48.902823
1301.613435	163.009327	48.907828
1298.081896	171.341160	48.912833
1294.455849	173.689055	48.917837
1290.922567	175.293168	48.922842
1287.608214	173.478739	48.927847
1283.923807	163.282061	48.932852
1280.294352	165.671369	48.937857
1276.609757	178.047606	48.942861
1273.380063	173.394010	48.947866
1269.911864	174.027965	48.952871
1266.481688	168.355997	48.957876
1263.364349	172.626294	48.962881
1259.581099	176.975931	48.967885
1256.129438	163.502681	48.972890
1252.534395	172.160714	48.977895
1248.925434	171.506290	48.982900
1245.383717	175.494249	48.987905
1241.770743	161.014518	48.992909
1238.842794	172.705206	48.997914
1235.310326	173.526282	49.002919
1231.431646	163.424846	49.007924
1227.422621	170.487600	49.012929
1224.304759	171.667616	49.017933
1221.294856	165.902522	49.022938
1217.344791	162.367253	49.027943
1214.013692	169.472105	49.032948
1210.519150	162.584311	49.037953
1206.925954	180.530571	49.042957
1203.886248	172.640430	49.047962
1199.543924	165.267805	49.052967
1196.398809	159.547047	49.057972
1193.036111	165.868964	49.062977
1189.563292	167.246301	49.067981
1185.442468	160.839660	49.072986
1182.136441	163.847271	49.077991
1179.313186	157.191312	49.082996
1175.744224	169.701410	49.088001
1171.759539	172.910838	49.093005
1168.109870	171.145214	49.098010
1164.487701	168.376955	49.103015
1161.397630	176.984914	49.108020
1157.858261	168.932324	49.113025
1154.354785	164.531561	49.118029
1151.107219	163.103264	49.123034
1147.227754	183.833210	49.128039
1144.005482	180.802323	49.133044
1140.517005	166.557719	49.138049
1137.103078	171.077201	49.143053
1133.389127	168.427503	49.148058
1129.436034	175.077179	49.153063
1126.518931	171.824756	49.158068
1123.254975	172.829158	49.163073
1119.580656	171.060330	49.168077
1115.719272	167.198436	49.173082
1112.208374	183.019623	49.178087
1109.118702	169.705124	49.183092
1105.719601	165.378610	49.188097
1101.513123	180.768774	49.193101
1098.155951	167.101555	49.198106
1094.798195	172.835505	49.203111
1091.168669	170.923548	49.208116
1087.872707	173.950456	49.213121
1084.434299	171.324354	49.218125
1081.222547	167.262592	49.223130
1077.134237	171.841646	49.228135
1073.538624	161.472301	49.233140
1070.286589	166.230073	49.238145
1066.642747	168.029538	49.243149
1063.144157	167.144882	49.248154
1059.644308	169.719883	49.253159
1056.314877	168.936739	49.258164
1053.302643	159.739604	49.263169
1049.209888	176.365610	49.268173
1045.838541	163.804524	49.273178
1042.748353	166.690734	49.278183
1038.816146	173.523367	49.283188
1035.479130	170.188780	49.288193
1031.435942	171.589727	49.293197
1028.407010	170.723836	49.298202
1024.674190	165.127327	49.303207
1021.403407	162.821640	49.308212
1017.889666	160.676330	49.313217
1013.852698	172.632862	49.318221
1010.756700	162.576183	49.323226
1007.014231	164.925588	49.328231
1003.731329	165.959318	49.333236
1000.708023	163.716962	49.338241
996.606794	163.260660	49.343245
993.593658	163.317661	49.348250
989.906288	170.750264	49.353255
986.120483	170.459720	49.358260
982.669754	162.638453	49.363265
979.283359	166.517036	49.368269
976.058996	165.796594	49.373274
972.110292	163.770775	49.378279
968.566362	170.427262	49.383284
965.087785	167.463944	49.388289
961.340564	171.077636	49.393293
958.393936	160.481542	49.398298
954.668688	162.522596	49.403303
951.303010	164.510597	49.408308
947.761292	166.998744	49.413313
944.296430	166.055408	49.418317
940.605812	159.629496	49.423322
936.945471	160.644879	49.428327
933.711690	164.513476	49.433332
930.451597	168.883445	49.438337
926.478925	164.536210	49.443341
923.462338	158.852481	49.448346
920.080763	169.033765	49.453351
915.928469	166.979936	49.458356
912.718955	153.946104	49.463361
908.971518	163.745628	49.468365
905.326923	162.140220	49.473370
901.942430	166.821873	49.478375
898.733378	164.801133	49.483380
895.414871	159.033297	49.488385
892.000313	162.477357	49.493389
888.576653	159.407249	49.498394
884.630519	163.514642	49.503399
881.142310	159.652341	49.508404
877.637383	158.249412	49.513409
873.849363	165.114748	49.518413
870.304565	154.617184	49.523418
867.081715	165.859751	49.528423
863.985564	175.593785	49.533428
860.611131	165.751077	49.538433
856.412338	160.847620	49.543437
852.751981	166.294635	49.548442
849.496430	156.407349	49.553447
845.920093	148.176778	49.558452
842.579708	157.787175	49.563457
839.054314	171.208492	49.568461
835.851256	165.856199	49.573466
831.931413	158.014723	49.578471
828.927327	152.063007	49.583476
825.348575	158.887296	49.588481
821.360057	164.466749	49.593485
817.759156	153.848654	49.598490
814.600409	161.123898	49.603495
811.061569	165.410711	49.608500
807.868786	166.139410	49.613505
803.998853	161.591692	49.618509
800.765462	159.322465	49.623514
796.730234	159.435478	49.628519
793.237597	154.642360	49.633524
789.976669	155.053504	49.638529
786.677627	165.291649	49.643533
783.357931	141.401072	49.648538
779.862973	152.891432	49.653543
776.097639	168.065635	49.658548
772.558632	155.954957	49.663553
768.807678	155.035776	49.668557
765.558705	157.769070	49.673562
761.821673	149.469688	49.678567
758.468864	158.804457	49.683572
754.921423	153.429174	49.688577
751.516938	150.390111	49.693581
748.135941	150.073497	49.698586
744.423194	159.643615	49.703591
741.011521	154.639552	49.708596
737.429428	149.006693	49.713601
733.592810	155.730066	49.718605
730.723084	154.069106	49.723610
727.101283	156.425270	49.728615
723.674970	155.492950	49.733620
720.501467	157.988374	49.738625
716.203705	152.891127	49.743629
713.005533	151.074184	49.748634
709.082217	165.732690	49.753639
706.098396	153.610675	49.758644
702.997173	153.486427	49.763649
699.001908	162.097933	49.768653
695.472263	138.163671	49.773658
691.844407	146.144172	49.778663
688.205267	160.902056	49.783668
684.924231	154.775264	49.788673
681.250729	147.030046	49.793677
678.475850	145.948926	49.798682
674.460877	145.950741	49.803687
670.901803	154.683384	49.808692
667.603572	145.735255	49.813697
663.866087	158.941963	49.818701
660.584435	160.698791	49.823706
657.076617	156.059793	49.828711
653.079262	166.857960	49.833716
650.220972	150.189161	49.838721
646.427391	148.830185	49.843725
642.926824	144.385733	49.848730
639.505631	152.473007	49.853735
635.727630	158.023018	49.858740
632.331831	151.753023	49.863745
628.740447	153.782304	49.868749
625.504890	152.956746	49.873754
621.874553	161.116261	49.878759
618.261302	146.871130	49.883764
614.992123	153.485649	49.888769
611.207590	149.201272	49.893773
607.899140	149.588291	49.898778
604.175218	152.517403	49.903783
600.847047	148.015397	49.908788
597.398861	144.351755	49.913793
593.708908	162.399916	49.918797
590.618033	145.445987	49.923802
586.970591	157.363137	49.928807
583.436043	155.691002	49.933812
579.800811	144.362014	49.938817
576.265186	153.684432	49.943821
573.274904	159.125776	49.948826
569.617711	157.176067	49.953831
565.841086	155.715979	49.958836
562.832856	147.566962	49.963841
558.961325	161.348323	49.968845
555.423900	156.396607	49.973850
551.720525	161.323072	49.978855
548.224466	153.091264	49.983860
544.898178	145.434596	49.988865
541.138671	154.448225	49.993869
537.591370	146.890021	49.998874
534.052362	143.553460	50.003879
530.876023	157.165248	50.008884
527.417035	155.613945	50.013889
523.748071	149.391306	50.018893
520.248620	147.152657	50.023898
516.995368	151.658608	50.028903
513.337966	150.055836	50.033908
509.928194	153.185566	50.038913
505.979091	162.030362	50.043917
502.744963	143.736354	50.048922
499.188486	146.461568	50.053927
495.788531	154.534151	50.058932
492.394538	151.429569	50.063937
488.523448	151.845362	50.068941
485.191857	142.254596	50.073946
481.815629	148.135007	50.078951
478.392600	151.609569	50.083956
475.093093	146.118327	50.088961
470.990584	152.327567	50.093965
467.735480	143.085844	50.098970
464.614970	153.442499	50.103975
461.010309	163.519443	50.108980
457.540203	143.098091	50.113985
453.393013	153.686004	50.118989
450.091695	144.448078	50.123994
446.727446	141.707578	50.128999
443.134036	147.319435	50.134004
440.009747	141.154267	50.139009
436.011840	147.666676	50.144013
432.645023	148.269712	50.149018
429.228055	153.325912	50.154023
425.535846	153.742578	50.159028
422.020728	138.986828	50.164033
418.816353	133.438077	50.169037
415.475275	145.704728	50.174042
411.576160	143.275661	50.179047
407.782151	142.920511	50.184052
404.645936	141.853919	50.189057
400.787290	144.330474	50.194061
397.444338	142.498543	50.199066
393.974794	164.180413	50.204071
390.682425	146.628610	50.209076
387.800368	143.853570	50.214081
383.606619	154.137760	50.219085
380.433100	145.693452	50.224090
376.401262	147.226492	50.229095
373.118453	152.866097	50.234100
369.530942	155.860407	50.239105
365.579362	152.474799	50.244109
362.495546	144.140481	50.249114
359.328166	143.323724	50.254119
355.739615	150.570512	50.259124
352.365211	149.659807	50.264129
348.869228	147.255632	50.269133
345.351955	144.860404	50.274138
341.292900	147.389734	50.279143
338.023736	150.823062	50.284148
335.294495	139.348813	50.289153
331.131500	143.404140	50.294157
327.529821	145.164277	50.299162
324.171987	150.574989	50.304167
320.634002	152.138250	50.309172
316.811707	147.224371	50.314177
313.158425	152.675415	50.319181
310.173291	150.622425	50.324186
306.719160	151.118605	50.329191
303.392991	147.918476	50.334196
299.547056	150.578855	50.339201
296.188515	158.526103	50.344205
292.710381	146.496264	50.349210
289.138785	147.445841	50.354215
285.492397	156.791721	50.359220
282.089186	142.691485	50.364225
278.312405	142.003862	50.369229
274.863753	150.859713	50.374234
271.506261	148.020327	50.379239
267.862381	152.049614	50.384244
264.606837	145.283027	50.389249
261.172407	161.182233	50.394253
257.523747	148.613229	50.399258
253.843466	139.245859	50.404263
250.369573	155.871366	50.409268
247.299795	145.246309	50.414273
243.330890	156.197227	50.419277
240.271389	151.322712	50.424282
236.801132	148.766074	50.429287
233.070749	153.559049	50.434292
229.412189	156.896256	50.439297
226.115478	159.028894	50.444301
222.435797	144.974672	50.449306
218.862558	146.464790	50.454311
215.406367	140.539562	50.459316
212.203043	137.306068	50.464321
208.486064	147.087559	50.469325
204.779500	146.651588	50.474330
201.284700	140.760469	50.479335
197.809937	149.428588	50.484340
195.007831	149.955212	50.489345
190.953622	147.636457	50.494349
187.606355	137.875331	50.499354
184.039944	144.842508	50.504359
180.368734	149.569204	50.509364
177.095312	138.165622	50.514369
173.171636	141.130736	50.519373
170.008472	148.330806	50.524378
166.476864	135.123285	50.529383
162.842719	151.941629	50.534388
159.637508	144.898447	50.539393
155.767469	143.678580	50.544397
152.544956	125.933607	50.549402
148.904626	144.092002	50.554407
145.280990	144.112253	50.559412
142.184757	137.873065	50.564417
138.642144	137.892560	50.569421
134.941776	143.479626	50.574426
131.503994	148.705737	50.579431
128.039119	144.375162	50.584436
124.158173	150.207238	50.589441
120.654042	139.995573	50.594445
116.896590	145.484351	50.599450
113.987586	146.989861	50.604455
110.845835	145.317313	50.609460
107.454983	139.353633	50.614465
103.341656	147.220778	50.619469
99.906174	144.006074	50.624474
96.307231	138.897588	50.629479
92.239405	153.720032	50.634484
89.042582	143.655111	50.639489
85.922551	145.914990	50.644493
82.496295	136.609546	50.649498
78.960206	134.218767	50.654503
75.348545	146.970754	50.659508
72.281032	144.239041	50.664513
68.277523	144.355751	50.669517
64.849676	144.397856	50.674522
61.764401	144.077821	50.679527
57.927854	136.092410	50.684532
54.354614	147.909033	50.689537
50.537356	145.648588	50.694541
47.110972	138.737127	50.699546
43.721890	137.771105	50.704551
40.087915	143.091142	50.709556
36.952881	130.428258	50.714561
33.490508	151.121115	50.719565
30.259833	132.307370	50.724570
26.374556	134.801860	50.729575
22.427255	145.555064	50.734580
19.620400	131.260380	50.739585
15.948336	133.522530	50.744589
12.166378	135.515268	50.749594
8.835436	138.792432	50.754599
5.073836	138.313586	50.759604
1.725559	129.702365	50.764609