Thu Jun 16 11:25:58 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.022689	79.552498	0.000000
-0.260262	89.886838	0.005005
0.448536	97.534813	0.010010
0.436188	91.716760	0.015014
-0.097175	83.774379	0.020019
0.131297	77.198731	0.025024
-0.085208	84.043069	0.030029
-0.305677	64.923233	0.035034
-0.434098	56.589968	0.040038
-0.850693	42.760998	0.045043
-1.265659	40.851557	0.050048
-1.345239	30.765945	0.055053
-1.660119	21.069345	0.060058
-2.189626	22.000022	0.065062
-2.415364	1.598052	0.070067
-2.533795	8.500336	0.075072
-3.241607	9.146466	0.080077
-3.401837	-5.333122	0.085082
-3.335433	-1.002098	0.090086
-3.790821	-4.633748	0.095091
-4.124082	-10.448350	0.100096
-4.810052	-10.599395	0.105101
-4.841778	-11.670969	0.110106
-4.980778	-2.372462	0.115110
-4.950795	-6.793640	0.120115
-4.948161	-0.466389	0.125120
-5.628860	6.105790	0.130125
-6.246929	-7.408182	0.135130
-6.487295	-4.678309	0.140134
-6.540320	2.546610	0.145139
-6.274765	-8.441766	0.150144
-6.435216	0.114570	0.155149
-7.236613	-5.746972	0.160154
-7.906910	-7.248010	0.165158
-8.025994	1.288665	0.170163
-7.987584	2.318846	0.175168
-8.162892	5.896251	0.180173
-8.149066	-1.536307	0.185178
-8.024715	0.663902	0.190182
-9.112908	1.637680	0.195187
-9.414656	-3.639146	0.200192
-9.609188	9.568005	0.205197
-9.522441	0.334813	0.210202
-9.426986	-0.354584	0.215206
-10.285805	4.408434	0.220211
-10.400288	-9.367420	0.225216
-10.782364	-17.280291	0.230221
-10.644488	-5.207351	0.235226
-10.860566	12.836869	0.240230
-11.790441	2.200930	0.245235
-12.008900	-11.306963	0.250240
-12.295699	-5.981353	0.255245
-12.304456	-8.927381	0.260250
-12.749857	-2.719547	0.265254
-12.851009	-0.889804	0.270259
-12.722499	-15.863602	0.275264
-12.772935	-5.846052	0.280269
-13.026977	-4.757774	0.285274
-13.570720	-1.383477	0.290278
-13.752917	-2.702762	0.295283
-14.128511	2.910202	0.300288
-14.644475	-0.957083	0.305293
-15.239941	-7.430466	0.310298
-15.230313	1.724603	0.315302
-15.255650	-4.229380	0.320307
-15.561199	-12.680425	0.325312
-16.077528	2.871905	0.330317
-15.881526	3.267846	0.335322
-16.252623	-7.835805	0.340326
-16.586070	-10.773553	0.345331
-16.075269	0.124855	0.350336
-17.003889	-2.140671	0.355341
-17.471681	-2.904694	0.360346
-17.833647	-0.986468	0.365350
-17.840622	3.917131	0.370355
-17.592214	-7.008332	0.375360
-17.821291	-2.180395	0.380365
-17.967829	-5.418850	0.385370
-18.974313	-5.724293	0.390374
-19.244496	-12.769063	0.395379
-19.353080	-14.377333	0.400384
-19.368523	1.438193	0.405389
-19.327381	-14.140017	0.410394
-20.026306	-1.281324	0.415398
-20.576937	-2.459910	0.420403
-20.815664	-7.937153	0.425408
-21.383174	-1.757084	0.430413
-20.998934	-8.807507	0.435418
-21.012601	-0.158034	0.440422
-21.395412	-10.118034	0.445427
-21.160604	-6.517648	0.450432
-21.893881	3.421468	0.455437
-22.427900	-11.089762	0.460442
-22.579734	-10.133503	0.465446
-22.638802	2.418098	0.470451
-22.403084	-20.614818	0.475456
-23.316128	-2.636266	0.480461
-23.666598	-2.135512	0.485466
-23.908550	-5.915489	0.490470
-24.134243	-0.127921	0.495475
-23.847199	7.106797	0.500480
-24.517770	1.325642	0.505485
-24.555922	-11.740090	0.510490
-25.252692	-3.392957	0.515494
-25.729365	-2.492617	0.520499
-25.821920	-14.954477	0.525504
-26.001193	-1.506680	0.530509
-25.779695	-1.402034	0.535514
-25.550033	-9.192754	0.540518
-26.148830	-6.406111	0.545523
-26.504880	-5.433268	0.550528
-27.314615	-1.074651	0.555533
-27.027720	1.264926	0.560538
-27.101555	-2.803379	0.565542
-28.244602	-11.544957	0.570547
-28.401880	-4.249244	0.575552
-28.670960	9.111692	0.580557
-28.639164	-9.889817	0.585562
-28.935688	-8.323450	0.590566
-29.270829	-2.264948	0.595571
-28.665165	-4.747039	0.600576
-28.997042	2.437740	0.605581
-29.495373	-13.052596	0.610586
-29.625750	-7.200579	0.615590
-30.356864	-0.163700	0.620595
-30.379613	-8.117905	0.625600
-30.476502	2.931838	0.630605
-31.448505	-10.192258	0.635610
-31.657339	1.068851	0.640614
-32.131342	-1.088902	0.645619
-31.884494	-8.403206	0.650624
-31.877535	-7.352833	0.655629
-32.128387	2.690937	0.660634
-32.348466	4.462300	0.665638
-32.272225	0.583468	0.670643
-32.836991	-3.728468	0.675648
-33.159764	9.492179	0.680653
-33.721286	9.218562	0.685658
-33.568979	-4.117688	0.690662
-33.795964	-4.026330	0.695667
-33.966154	-3.048589	0.700672
-35.131091	5.146652	0.705677
-35.541528	-0.940106	0.710682
-35.514349	-4.956638	0.715686
-35.351232	-6.547857	0.720691
-35.482800	-6.874673	0.725696
-35.435471	-2.107413	0.730701
-35.450805	-4.355568	0.735706
-35.678165	-0.493629	0.740710
-36.563998	-1.903107	0.745715
-36.355842	0.815583	0.750720
-36.833289	-1.538216	0.755725
-36.890113	-0.689997	0.760730
-38.097238	3.379245	0.765734
-38.220958	-2.763578	0.770739
-38.136762	-3.677326	0.775744
-38.617241	9.437090	0.780749
-38.474925	1.642648	0.785754
-38.424287	-7.234646	0.790758
-38.244037	-7.621973	0.795763
-39.301846	-0.613873	0.800768
-39.485742	17.302502	0.805773
-40.064538	0.086396	0.810778
-39.917813	-7.357467	0.815782
-40.203226	-0.544397	0.820787
-40.478754	-4.552139	0.825792
-41.182806	-1.372921	0.830797
-41.814904	-4.297518	0.835802
-41.597854	-5.796433	0.840806
-41.689921	-9.396079	0.845811
-41.710172	-5.150475	0.850816
-41.786558	-5.022644	0.855821
-41.795284	-4.496486	0.860826
-41.857291	-0.266670	0.865830
-42.781657	-3.329024	0.870835
-43.103286	-7.794887	0.875840
-43.313060	-1.159661	0.880845
-43.117946	-12.570759	0.885850
-43.569530	-3.265285	0.890854
-44.530575	-3.792804	0.895859
-44.426241	3.447344	0.900864
-44.478517	4.440324	0.905869
-44.811224	-8.163372	0.910874
-44.862375	-0.566154	0.915878
-44.982910	0.938969	0.920883
-45.628391	-16.842526	0.925888
-46.406979	-1.690502	0.930893
-46.083476	-11.083662	0.935898
-46.053629	-12.752199	0.940902
-46.460240	2.571174	0.945907
-46.305493	-12.242701	0.950912
-46.704636	-19.419162	0.955917
-47.501040	-15.297643	0.960922
-47.737968	-12.575738	0.965926
-47.936225	-9.960159	0.970931
-47.604210	-8.283394	0.975936
-48.502250	-7.402596	0.980941
-48.998485	-5.846432	0.985946
-49.172953	-7.951481	0.990950
-49.574430	-12.541075	0.995955
-49.471926	-18.192992	1.000960
-49.637714	-4.685870	1.005965
-49.516025	-10.642344	1.010970
-49.422270	-10.388338	1.015974
-49.809152	-5.770005	1.020979
-50.546973	-11.769601	1.025984
-50.933390	-7.533330	1.030989
-50.889235	-11.068181	1.035994
-51.007574	-10.007261	1.040998
-51.823691	1.640896	1.046003
-52.294452	-16.849488	1.051008
-52.490500	-4.148884	1.056013
-52.703016	3.780828	1.061018
-52.895017	-7.546761	1.066022
-53.138063	-3.533955	1.071027
-52.581179	-6.699051	1.076032
-52.755261	-5.549404	1.081037
-53.212955	-11.876063	1.086042
-53.540363	-10.430866	1.091046
-54.192500	0.459171	1.096051
-54.290587	-9.987182	1.101056
-54.688407	-9.233942	1.106061
-54.574459	-5.704048	1.111066
-54.830568	-8.419288	1.116070
-55.714494	-4.256467	1.121075
-55.779358	-7.195491	1.126080
-56.242649	-3.751127	1.131085
-56.015106	0.557012	1.136090
-56.051339	-6.774632	1.141094
-56.248557	3.230578	1.146099
-56.304093	-1.378507	1.151104
-57.052057	2.919986	1.156109
-57.488197	-9.520111	1.161114
-57.546159	-9.175033	1.166118
-57.850930	-3.346874	1.171123
-57.779231	-16.659035	1.176128
-58.513545	-5.229009	1.181133
-59.275637	1.635416	1.186138
-59.477254	-10.130870	1.191142
-59.143263	-11.482585	1.196147
-59.067533	-5.338090	1.201152
-59.432044	4.405321	1.206157
-59.502249	-4.500933	1.211162
-59.416814	-11.462411	1.216166
-60.623666	-1.491989	1.221171
-60.850661	-5.162859	1.226176
-61.115613	-8.208013	1.231181
-61.101598	-8.900820	1.236186
-60.864857	-7.994278	1.241190
-60.907525	-2.696783	1.246195
-62.034041	-8.336179	1.251200
-62.233025	-0.118370	1.256205
-62.060713	1.256669	1.261210
-62.292664	-6.088403	1.266214
-62.933927	-1.717672	1.271219
-63.448947	-4.231489	1.276224
-64.032246	-4.591770	1.281229
-63.675213	-0.603459	1.286234
-64.254448	-3.285718	1.291238
-64.154908	-2.221543	1.296243
-63.870654	-4.285600	1.301248
-64.083461	3.467275	1.306253
-64.236164	-7.624417	1.311258
-65.039495	-4.067030	1.316262
-65.549552	4.444583	1.321267
-65.699177	-13.226586	1.326272
-66.139357	-6.091391	1.331277
-66.296119	-0.803648	1.336282
-65.821665	-13.355859	1.341286
-66.565370	4.684783	1.346291
-67.358415	-7.965257	1.351296
-67.414303	-5.643318	1.356301
-67.606413	-3.677397	1.361306
-67.771209	-1.236043	1.366310
-68.031752	13.023000	1.371315
-67.708075	-2.445050	1.376320
-67.857538	7.123424	1.381325
-68.572136	2.486727	1.386330
-68.831171	-2.154921	1.391334
-69.452486	6.222662	1.396339
-69.289812	-4.653706	1.401344
-69.584832	-0.146246	1.406349
-69.589326	-1.556951	1.411354
-69.824960	-2.666447	1.416358
-70.554478	2.534338	1.421363
-70.838197	-2.409646	1.426368
-70.935258	1.583276	1.431373
-70.975583	10.044486	1.436378
-70.757060	2.743739	1.441382
-71.773209	8.930285	1.446387
-72.007253	-2.573260	1.451392
-72.371871	5.136635	1.456397
-72.876539	3.919086	1.461402
-72.805882	-1.751348	1.466406
-72.983300	0.330825	1.471411
-72.940346	-2.990244	1.476416
-72.715029	-4.612066	1.481421
-73.513561	2.599228	1.486426
-73.707925	-0.956086	1.491430
-74.345045	-3.756927	1.496435
-74.302019	6.234327	1.501440
-74.091062	8.154548	1.506445
-74.667257	-1.954614	1.511450
-75.003676	-1.493174	1.516454
-75.534544	-5.183076	1.521459
-75.317654	-10.336858	1.526464
-75.733907	0.525933	1.531469
-76.616232	-2.685226	1.536474
-76.896255	-11.615101	1.541478
-77.285987	2.528451	1.546483
-76.702026	2.313535	1.551488
-77.350827	0.613323	1.556493
-77.023154	-11.030996	1.561498
-77.092379	-6.072129	1.566502
-77.701453	-4.373702	1.571507
-78.180751	-5.982853	1.576512
-78.329903	-2.303918	1.581517
-78.817710	0.355670	1.586522
-79.148871	-4.899515	1.591526
-79.190202	-2.580673	1.596531
-79.059309	-5.578685	1.601536
-79.357029	-7.818543	1.606541
-80.156169	-1.237246	1.611546
-80.334552	-3.432803	1.616550
-80.850237	-1.342965	1.621555
-80.654738	-4.453366	1.626560
-80.677972	-7.504334	1.631565
-80.654674	-4.690873	1.636570
-81.063644	-5.482864	1.641574
-82.032228	-4.489382	1.646579
-82.251808	1.737068	1.651584
-82.300071	-9.403154	1.656589
-82.541962	-19.219113	1.661594
-82.197318	-14.414380	1.666598
-82.462708	-1.406061	1.671603
-82.900736	-9.925964	1.676608
-83.459145	-6.997026	1.681613
-84.012937	0.122124	1.686618
-83.620074	-5.508529	1.691622
-84.000791	-3.404496	1.696627
-84.304172	-5.681894	1.701632
-85.387233	-10.143052	1.706637
-85.454666	-11.408890	1.711642
-85.378569	-5.837632	1.716646
-85.169566	-5.771765	1.721651
-85.246552	-6.302441	1.726656
-85.893090	-2.116305	1.731661
-86.034999	-0.135200	1.736666
-85.970605	-5.908478	1.741670
-86.903467	-4.998342	1.746675
-86.978708	-7.213805	1.751680
-87.053812	-12.831632	1.756685
-87.613588	-0.460198	1.761690
-87.339726	-15.913883	1.766694
-87.929483	1.303208	1.771699
-88.613218	-1.718408	1.776704
-88.666304	-3.631512	1.781709
-88.803781	8.252832	1.786714
-88.839178	-0.651972	1.791718
-88.988869	-0.615808	1.796723
-88.806777	-1.957809	1.801728
-88.951873	-8.564806	1.806733
-90.277763	1.239926	1.811738
-90.178103	0.180969	1.816742
-90.518741	7.081498	1.821747
-90.370553	-4.879630	1.826752
-90.468925	2.713552	1.831757
-91.298300	9.494691	1.836762
-91.715246	-3.135722	1.841766
-92.208652	-2.159707	1.846771
-91.993361	1.467578	1.851776
-92.024216	6.769733	1.856781
-92.197950	-1.811809	1.861786
-92.167218	-4.833616	1.866790
-93.264827	6.115252	1.871795
-93.471321	-14.813405	1.876800
-93.264503	-1.546429	1.881805
-93.566621	4.191618	1.886810
-93.510935	-2.770075	1.891814
-94.031054	-5.084555	1.896819
-94.623448	-3.325745	1.901824
-94.991456	-6.382671	1.906829
-95.244067	-4.079814	1.911834
-94.997307	-4.367052	1.916838
-95.413206	0.919620	1.921843
-95.214604	-6.598912	1.926848
-95.535005	-3.186350	1.931853
-96.406191	3.722152	1.936858
-96.739198	-6.670770	1.941862
-96.917571	0.091065	1.946867
-96.776219	-6.313485	1.951872
-96.779931	5.469924	1.956877
-97.364893	1.095729	1.961882
-98.322104	0.973345	1.966886
-98.387530	-5.241751	1.971891
-98.224377	2.286010	1.976896
-98.862562	10.186535	1.981901
-98.696432	3.299419	1.986906
-98.395736	-4.912055	1.991910
-98.537516	3.278048	1.996915
-98.994501	-6.196170	2.006912
-99.501162	-1.969766	2.016909
-98.733596	1.605533	2.026906
-98.379543	-1.697231	2.036902
-97.350657	-9.201136	2.046899
-97.065128	-3.048832	2.056896
-96.900147	-2.993954	2.066893
-95.586092	-2.358709	2.076890
-95.514677	-3.537776	2.086886
-95.481389	3.464926	2.096883
-94.891783	1.579287	2.106880
-94.079134	-6.175933	2.116877
-93.727823	2.048953	2.126874
-92.855687	-2.733459	2.136870
-92.540107	-4.670512	2.146867
-92.477098	0.170925	2.156864
-91.566394	3.185605	2.166861
-91.176129	1.665848	2.176858
-90.768762	3.026287	2.186854
-89.861706	-7.611555	2.196851
-89.407582	0.971502	2.206848
-89.346103	4.614112	2.216845
-88.642821	3.922745	2.226842
-88.103317	0.241530	2.236838
-87.741017	-0.165696	2.246835
-87.047904	-1.116209	2.256832
-86.632329	-6.416924	2.266829
-86.198356	4.558592	2.276826
-85.487781	2.115453	2.286822
-85.142902	0.277572	2.296819
-84.525869	1.040268	2.306816
-83.657339	4.032235	2.316813
-83.682968	3.366659	2.326810
-83.344764	-1.790042	2.336806
-82.648521	-8.733910	2.346803
-82.071044	1.424639	2.356800
-81.918734	1.182903	2.366797
-80.791923	-4.810059	2.376794
-80.623003	-1.101294	2.386790
-80.372043	-4.918401	2.396787
-79.088938	-0.386578	2.406784
-78.770639	-10.884143	2.416781
-78.858982	-0.355664	2.426778
-78.425185	-2.840230	2.436774
-77.536668	0.631565	2.446771
-77.131861	-0.477993	2.456768
-76.110218	-6.411542	2.466765
-75.810771	-4.014605	2.476762
-75.606842	-9.191142	2.486758
-75.784816	5.001209	2.496755
-74.469391	10.527935	2.506752
-74.266793	3.852043	2.516749
-73.258532	4.142222	2.526746
-72.757685	9.513114	2.536742
-72.459779	4.334030	2.546739
-72.449134	10.456750	2.556736
-71.491177	-2.926684	2.566733
-71.148696	2.109439	2.576730
-70.756982	-4.415456	2.586726
-69.796074	-9.138007	2.596723
-69.453701	1.827806	2.606720
-69.363515	-3.458250	2.616717
-68.537335	-2.413580	2.626714
-68.249662	-1.355921	2.636710
-67.238999	-1.130840	2.646707
-66.680092	1.407787	2.656704
-66.491699	1.230122	2.666701
-66.264543	-5.524699	2.676698
-65.806592	-7.441373	2.686694
-64.526992	4.808020	2.696691
-64.581749	2.194340	2.706688
-64.242221	-8.111154	2.716685
-63.857159	-1.333230	2.726682
-63.234849	-1.089353	2.736678
-62.126517	-5.134492	2.746675
-61.770946	-2.303013	2.756672
-61.737043	-2.939559	2.766669
-61.447055	-2.811252	2.776666
-60.459131	-4.550787	2.786662
-60.331062	-10.592688	2.796659
-59.214317	-0.797125	2.806656
-58.698128	-7.728374	2.816653
-58.562390	-7.468387	2.826650
-58.213747	0.111076	2.836646
-57.783916	-5.565035	2.846643
-57.144341	1.511419	2.856640
-56.215019	1.244887	2.866637
-55.794765	-5.912073	2.876634
-55.297879	-4.061664	2.886630
-55.133722	-1.098684	2.896627
-54.857201	-10.307981	2.906624
-53.836442	4.499509	2.916621
-53.662352	-11.105615	2.926618
-52.609814	-9.237047	2.936614
-52.027870	-0.569860	2.946611
-52.071270	-13.997203	2.956608
-52.016364	-5.814947	2.966605
-51.135073	-1.424096	2.976602
-50.465479	-4.273504	2.986598
-49.993581	-5.497175	2.996595
-49.161013	-0.549306	3.006592
-48.858227	-1.539617	3.016589
-49.042929	1.044859	3.026586
-48.000494	-4.776453	3.036582
-47.566735	-11.566059	3.046579
-46.790940	-6.339685	3.056576
-46.267461	-5.061009	3.066573
-45.698245	1.964499	3.076570
-45.719319	-4.332549	3.086566
-45.356800	-7.176744	3.096563
-44.441344	-15.456476	3.106560
-44.208293	-6.779044	3.116557
-42.991762	-1.446864	3.126554
-42.809242	-1.007174	3.136550
-42.528888	-3.193847	3.146547
-42.532983	-8.016208	3.156544
-41.493513	0.635475	3.166541
-41.159331	-1.180732	3.176538
-40.160599	1.044237	3.186534
-39.413488	-4.302380	3.196531
-39.301384	-1.492252	3.206528
-39.115486	-6.804052	3.216525
-38.969662	-3.881999	3.226522
-38.110977	-4.500215	3.236518
-37.931800	-11.787526	3.246515
-36.662272	-6.040144	3.256512
-36.283822	-7.070667	3.266509
-36.228947	-5.233787	3.276506
-35.194419	-5.676540	3.286502
-34.949876	-0.630006	3.296499
-34.620149	-9.758208	3.306496
-33.703858	-4.176626	3.316493
-33.220189	-7.163724	3.326490
-33.148307	-8.050975	3.336486
-32.603313	-1.863607	3.346483
-31.632633	-5.704139	3.356480
-31.568222	-4.552191	3.366477
-31.254796	-5.615380	3.376474
-30.223343	-6.473189	3.386470
-30.049898	-6.024590	3.396467
-29.655597	-10.247563	3.406464
-28.739693	-5.958048	3.416461
-28.529985	-6.683607	3.426458
-28.016465	-0.151087	3.436454
-27.039021	-6.841089	3.446451
-26.571711	-6.136964	3.456448
-26.776147	0.708064	3.466445
-26.398447	-6.833819	3.476442
-25.287025	-5.275415	3.486438
-25.110130	-7.805188	3.496435
-24.229510	-2.507082	3.506432
-23.722953	-2.687344	3.516429
-23.657182	-3.591317	3.526426
-23.037448	6.219920	3.536422
-22.174044	-6.546663	3.546419
-21.889130	-8.870454	3.556416
-21.575678	0.935587	3.566413
-20.686821	0.503081	3.576410
-20.498259	3.026414	3.586406
-20.204628	4.463046	3.596403
-19.039408	-1.816248	3.606400
-18.524315	3.016071	3.616397
-18.727888	-1.062559	3.626394
-18.260913	3.704863	3.636390
-17.348038	-0.766256	3.646387
-16.926261	2.713934	3.656384
-16.383877	-5.306835	3.666381
-15.648805	-3.457360	3.676378
-15.487526	0.083809	3.686374
-15.116449	-0.265546	3.696371
-14.186977	6.949257	3.706368
-13.894190	1.359356	3.716365
-13.919277	-1.104441	3.726362
-12.899291	-2.674823	3.736358
-12.566651	-2.710524	3.746355
-11.548376	-2.315012	3.756352
-11.261197	-3.243178	3.766349
-10.985073	-0.864113	3.776346
-10.925852	-7.839612	3.786342
-9.735577	-5.574283	3.796339
-9.328605	0.203097	3.806336
-8.596902	2.082419	3.816333
-8.157442	-3.431360	3.826330
-7.798286	0.540630	3.836326
-7.613816	1.124464	3.846323
-7.210099	2.078245	3.856320
-6.400586	-5.254665	3.866317
-5.920070	-5.109491	3.876314
-5.101936	-2.609253	3.886310
-4.357905	-5.456339	3.896307
-4.404726	1.480387	3.906304
-4.070201	5.175571	3.916301
-3.970347	20.339558	3.926298
-3.456195	25.068521	3.936294
-2.677104	34.407801	3.946291
-2.457871	56.428392	3.956288
-1.830210	64.429260	3.966285
-1.497115	87.903936	3.976282
-1.005970	99.494080	3.986278
-0.239531	125.300666	3.996275
0.000000	140.740591	4.001280
-0.069427	146.919203	4.006285
0.080369	156.610866	4.011290
0.194537	155.069056	4.016294
0.571472	172.585135	4.021299
0.517716	169.404509	4.026304
0.797204	170.890303	4.031309
0.916506	173.397200	4.036314
0.989529	168.022765	4.041318
0.780588	166.601239	4.046323
0.743389	168.384622	4.051328
1.084499	186.476266	4.056333
0.931138	172.770698	4.061338
0.921521	165.371923	4.066342
0.724226	180.832051	4.071347
0.845461	187.124290	4.076352
1.243579	198.441114	4.081357
1.246649	204.748055	4.086362
0.853577	179.568935	4.091366
0.721435	188.061405	4.096371
0.769279	192.703747	4.101376
1.225257	202.989053	4.106381
0.627757	197.274173	4.111386
1.330332	195.812993	4.116390
1.153271	204.270277	4.121395
1.307558	200.125842	4.126400
1.413814	204.499665	4.131405
1.187502	201.903368	4.136410
1.301877	192.057193	4.141414
0.962384	181.603737	4.146419
1.048690	189.348810	4.151424
1.089347	204.881808	4.156429
1.111471	194.786087	4.161434
1.183967	205.554345	4.166438
1.174107	204.277888	4.171443
1.169561	192.712779	4.176448
0.989460	200.022128	4.181453
1.065931	206.686005	4.186458
1.148208	196.559921	4.191462
1.237083	207.766853	4.196467
1.285240	212.254262	4.201472
1.402840	195.284505	4.206477
1.100304	205.879944	4.211482
1.477367	204.662664	4.216486
1.110325	207.817005	4.221491
1.041968	187.757747	4.226496
0.975482	200.988789	4.231501
1.084567	214.502083	4.236506
1.219882	189.871847	4.241510
1.180501	203.274116	4.246515
1.485848	223.762109	4.251520
1.773910	233.358361	4.256525
1.549785	223.290985	4.261530
1.591118	209.666860	4.266534
1.418908	206.617973	4.271539
1.555432	204.131892	4.276544
1.460065	202.619083	4.281549
1.396756	210.077637	4.286554
1.537391	193.051986	4.291558
1.348234	205.768895	4.296563
1.099147	201.877282	4.301568
1.768847	217.301009	4.306573
1.818351	222.304457	4.311578
1.610353	214.657080	4.316582
1.565740	216.805630	4.321587
1.604416	195.377600	4.326592
1.517922	210.472578	4.331597
1.303019	221.599598	4.336602
1.833146	223.758135	4.341606
1.954176	242.510502	4.346611
1.804377	230.440481	4.351616
1.509987	203.757796	4.356621
1.241093	206.857343	4.361626
1.873959	223.424255	4.366630
1.885418	234.282727	4.371635
1.702454	226.428769	4.376640
2.033333	221.021864	4.381645
1.635962	220.255561	4.386650
1.654704	211.448816	4.391654
2.096682	222.809019	4.396659
1.575121	222.553750	4.401664
1.707066	210.062100	4.406669
1.873130	226.438312	4.411674
2.082883	227.447887	4.416678
1.639284	216.483316	4.421683
1.967642	209.460379	4.426688
1.704716	215.025796	4.431693
1.931395	222.039546	4.436698
1.964701	213.223684	4.441702
1.859799	222.322146	4.446707
1.783436	218.868817	4.451712
2.002092	224.291216	4.456717
1.737587	242.159225	4.461722
2.078383	238.989741	4.466726
2.064164	245.597295	4.471731
2.000958	235.635811	4.476736
1.990641	227.060370	4.481741
2.088116	229.073171	4.486746
2.178293	239.266730	4.491750
1.678258	226.855928	4.496755
1.919936	232.563288	4.501760
2.188331	231.036826	4.506765
1.746528	240.688292	4.511770
2.128365	242.789850	4.516774
2.146021	242.021748	4.521779
2.092537	239.388300	4.526784
2.259142	242.156225	4.531789
1.697939	255.609852	4.536794
1.867643	246.967654	4.541798
2.019671	237.616491	4.546803
2.480059	246.020543	4.551808
2.470264	228.340772	4.556813
1.982870	232.260935	4.561818
2.670444	242.987060	4.566822
2.158961	242.164143	4.571827
2.208793	227.810723	4.576832
2.401707	236.751653	4.581837
1.958489	240.235074	4.586842
2.089167	238.294429	4.591846
2.194266	244.421942	4.596851
2.247018	243.865375	4.601856
2.280248	235.165532	4.606861
2.082586	237.112176	4.611866
2.379604	227.064925	4.616870
1.992214	244.103434	4.621875
1.852261	239.813560	4.626880
2.193090	233.717976	4.631885
1.789784	246.739340	4.636890
1.807789	252.795222	4.641894
2.401252	263.850144	4.646899
2.642763	264.057145	4.651904
2.701380	265.485629	4.656909
2.546594	276.634619	4.661914
2.814677	269.190099	4.666918
2.300229	266.465310	4.671923
2.394429	258.736400	4.676928
2.589747	265.313972	4.681933
2.248328	268.325481	4.686938
2.290923	258.542524	4.691942
2.447143	265.218108	4.696947
2.364804	266.342253	4.701952
3.042044	250.848363	4.706957
2.560123	269.491455	4.711962
2.872242	270.452448	4.716966
2.693726	265.768204	4.721971
2.380870	277.609632	4.726976
2.792724	265.243338	4.731981
2.715453	267.320934	4.736986
2.508712	251.054358	4.741990
2.609882	261.215333	4.746995
2.655826	271.294877	4.752000
2.793311	271.190747	4.757005
2.723947	277.273212	4.762010
2.839802	269.341535	4.767014
2.801565	271.738833	4.772019
2.461497	251.602851	4.777024
2.560058	253.249171	4.782029
2.506375	262.426007	4.787034
3.078264	260.137791	4.792038
2.875343	275.485786	4.797043
2.479897	271.480521	4.802048
2.768843	267.271689	4.807053
2.635017	270.640748	4.812058
3.161227	267.870949	4.817062
2.771192	270.371963	4.822067
2.451532	271.423848	4.827072
2.385782	271.710534	4.832077
2.344465	263.749685	4.837082
2.618083	272.213917	4.842086
2.431109	277.786437	4.847091
2.600465	278.945742	4.852096
2.967378	290.874519	4.857101
2.614940	304.185265	4.862106
2.720171	294.767908	4.867110
2.805452	295.435995	4.872115
3.071386	302.437375	4.877120
3.326646	293.002921	4.882125
3.027420	300.176425	4.887130
3.192296	296.614646	4.892134
2.957630	298.041681	4.897139
2.764647	291.939089	4.902144
3.170458	289.688377	4.907149
3.334976	306.169898	4.912154
3.072888	288.403796	4.917158
3.089479	283.494729	4.922163
2.824416	287.179472	4.927168
3.343139	294.157423	4.932173
3.069073	299.333445	4.937178
3.237349	293.817835	4.942182
3.204311	297.608667	4.947187
3.043468	299.073717	4.952192
3.151636	291.280034	4.957197
2.986533	299.519340	4.962202
3.128633	300.097140	4.967206
3.264188	297.162127	4.972211
2.899047	305.104296	4.977216
2.994838	292.726778	4.982221
2.926563	298.756488	4.987226
3.000771	295.742628	4.992230
2.747087	306.484063	4.997235
2.779592	322.858673	5.002240
3.360460	327.107631	5.007245
3.260923	329.673311	5.012250
3.231275	323.853195	5.017254
3.348951	330.106324	5.022259
3.397561	319.521550	5.027264
3.539246	327.441533	5.032269
3.264665	325.086413	5.037274
3.729227	323.973938	5.042278
3.570070	329.598114	5.047283
3.562059	333.511886	5.052288
3.591404	320.788984	5.057293
3.409389	324.920731	5.062298
3.409476	331.909529	5.067302
3.180966	329.444194	5.072307
3.334327	328.623373	5.077312
3.650562	330.382995	5.082317
3.395870	334.337830	5.087322
3.618412	328.762234	5.092326
3.705332	330.464056	5.097331
3.345972	334.759877	5.102336
3.806509	327.918765	5.107341
3.612513	334.537224	5.112346
3.697066	326.720296	5.117350
3.600698	328.960186	5.122355
3.351304	342.470583	5.127360
3.507175	326.337958	5.132365
3.610914	337.724252	5.137370
3.958567	332.481856	5.142374
3.776232	339.335853	5.147379
3.459612	336.418339	5.152384
3.950670	329.369150	5.157389
3.312262	343.422709	5.162394
3.414174	338.075307	5.167398
3.713536	342.063479	5.172403
3.828461	340.655795	5.177408
3.771562	340.319886	5.182413
3.815573	334.785729	5.187418
3.966018	326.235756	5.192422
3.744855	326.383075	5.197427
3.411581	330.796029	5.202432
3.841154	322.277077	5.207437
3.456414	327.621848	5.212442
3.500772	331.153556	5.217446
3.882550	337.187633	5.222451
3.541245	329.470578	5.227456
3.704643	337.100286	5.232461
3.031743	337.560414	5.237466
3.850811	340.554676	5.242470
3.831606	356.315551	5.247475
3.423449	368.049380	5.252480
3.868474	354.020517	5.257485
3.931351	357.945469	5.262490
3.830770	367.206872	5.267494
3.960913	353.613225	5.272499
4.130711	364.334537	5.277504
4.201700	358.526091	5.282509
4.075264	363.164828	5.287514
3.991336	360.940779	5.292518
3.848249	356.602063	5.297523
3.939409	357.314759	5.302528
4.117932	361.849924	5.307533
3.829507	369.918749	5.312538
3.892453	364.468762	5.317542
3.822895	359.973758	5.322547
3.825865	358.121388	5.327552
3.669457	365.013830	5.332557
3.912582	374.606251	5.337562
4.493918	386.463954	5.342566
4.275467	376.426419	5.347571
3.685385	364.891550	5.352576
4.048507	384.487245	5.357581
4.246946	392.093234	5.362586
4.507299	386.134801	5.367590
4.403458	389.786611	5.372595
4.196160	381.072963	5.377600
4.340829	366.888916	5.382605
3.830457	367.252534	5.387610
4.366249	384.497543	5.392614
4.711531	393.721486	5.397619
4.250288	382.943803	5.402624
4.308785	357.699925	5.407629
4.058977	367.360387	5.412634
4.295131	388.795784	5.417638
4.602569	387.583781	5.422643
4.410632	380.851855	5.427648
4.422156	380.422555	5.432653
4.082903	366.399873	5.437658
4.393067	372.885111	5.442662
4.427348	392.004690	5.447667
4.500762	400.744377	5.452672
4.307092	389.604503	5.457677
4.627203	399.241931	5.462682
4.409375	397.851152	5.467686
4.460664	393.759400	5.472691
4.398134	405.150333	5.477696
4.080882	394.876851	5.482701
3.899055	397.123771	5.487706
4.329495	390.488566	5.492710
4.505758	396.531276	5.497715
4.123361	398.963962	5.502720
4.606377	398.027789	5.507725
4.347860	399.782760	5.512730
4.394358	402.310309	5.517734
4.645047	400.125074	5.522739
4.315107	397.565107	5.527744
4.693946	391.429834	5.532749
4.715392	408.896508	5.537754
4.344551	420.674426	5.542758
5.055207	405.393085	5.547763
4.575013	408.302657	5.552768
4.556420	404.273553	5.557773
4.422596	411.794272	5.562778
5.129740	414.303508	5.567782
4.775902	412.784261	5.572787
4.662149	399.804463	5.577792
4.846669	400.368449	5.582797
4.712772	413.114774	5.587802
4.469211	394.127977	5.592806
4.959836	407.878400	5.597811
4.933271	421.042953	5.602816
5.017849	400.721171	5.607821
4.894464	397.857344	5.612826
4.733375	397.774439	5.617830
4.888705	398.449698	5.622835
4.487952	406.954419	5.627840
4.671427	415.494696	5.632845
5.026792	423.828201	5.637850
4.953439	424.124334	5.642854
5.055077	439.014318	5.647859
4.832741	429.427458	5.652864
4.875931	423.540218	5.657869
4.989493	424.519039	5.662874
5.026363	429.485574	5.667878
5.106136	426.992954	5.672883
4.774298	434.980690	5.677888
4.940236	433.009136	5.682893
4.953051	437.018642	5.687898
5.118892	428.801300	5.692902
5.164678	428.570555	5.697907
4.716785	434.650032	5.702912
4.943889	423.442471	5.707917
4.644107	433.053124	5.712922
4.814200	422.547846	5.717926
5.029101	437.821725	5.722931
4.898634	437.697157	5.727936
4.990725	430.927939	5.732941
4.596176	429.072984	5.737946
4.716572	435.042859	5.742950
5.166484	450.059292	5.747955
4.740838	463.031946	5.752960
5.321879	457.437804	5.757965
4.902881	460.016936	5.762970
5.177629	465.497533	5.767974
5.520771	461.980642	5.772979
5.299613	467.551678	5.777984
5.518742	459.478529	5.782989
5.259258	476.762529	5.787994
5.351778	458.793392	5.792998
5.476848	459.919481	5.798003
5.188176	463.565153	5.803008
5.198055	452.521920	5.808013
5.338504	463.915560	5.813018
5.365903	465.649332	5.818022
5.345791	459.125355	5.823027
5.186372	456.191508	5.828032
5.191532	465.405997	5.833037
5.346337	473.590161	5.838042
5.559002	460.924059	5.843046
5.500710	460.778487	5.848051
5.369683	457.345088	5.853056
5.770532	458.146505	5.858061
5.435288	462.341199	5.863066
5.505031	473.448589	5.868070
5.786847	457.670399	5.873075
5.276823	456.221848	5.878080
5.524080	452.205328	5.883085
5.299440	459.535676	5.888090
5.386092	463.883611	5.893094
5.380555	463.091115	5.898099
5.336566	466.530018	5.903104
5.310367	461.556439	5.908109
5.495359	463.645276	5.913114
4.932003	462.121089	5.918118
5.596535	461.421878	5.923123
5.512036	460.701723	5.928128
5.392355	443.274567	5.933133
5.473290	456.605477	5.938138
5.156511	458.718338	5.943142
5.764112	464.356532	5.948147
5.767709	480.413779	5.953152
5.906621	484.545412	5.958157
5.598765	469.622240	5.963162
5.533778	462.996070	5.968166
5.530166	483.902668	5.973171
5.814841	480.418620	5.978176
5.727116	480.429448	5.983181
5.886018	490.079763	5.988186
5.978421	486.354309	5.993190
5.705729	481.771097	5.998195
5.467666	488.977792	6.003200
5.712464	479.736543	6.008205
5.850413	492.359577	6.013210
5.922109	489.318470	6.018214
6.274067	490.028818	6.023219
5.744089	485.243160	6.028224
5.853899	479.440783	6.033229
6.249128	462.543533	6.038234
5.884556	458.743944	6.043238
5.833543	457.159948	6.048243
5.664903	461.803026	6.053248
5.634511	458.387921	6.058253
5.754308	458.552985	6.063258
5.531652	462.557313	6.068262
5.420074	463.543253	6.073267
5.841087	482.388008	6.078272
6.467108	478.342035	6.083277
6.012549	467.660462	6.088282
6.099944	470.883203	6.093286
6.281393	456.282191	6.098291
5.722686	469.449587	6.103296
5.786965	462.940075	6.108301
5.810659	463.254306	6.113306
5.794294	457.447434	6.118310
5.817994	454.555047	6.123315
5.595084	453.190754	6.128320
5.737584	453.484068	6.133325
5.722740	466.472595	6.138330
5.587417	455.481472	6.143334
5.900026	456.029423	6.148339
5.740444	461.973756	6.153344
5.930777	458.208152	6.158349
5.768473	453.890638	6.163354
5.810702	456.491512	6.168358
5.842044	456.088533	6.173363
5.809367	453.897141	6.178368
6.026587	457.347727	6.183373
5.957517	461.703440	6.188378
5.995709	449.961583	6.193382
6.054017	447.382828	6.198387
5.558795	461.550061	6.203392
5.829928	456.204151	6.208397
6.022326	460.179941	6.213402
5.883447	463.528469	6.218406
6.001239	461.616366	6.223411
5.490732	456.422221	6.228416
5.565324	462.739843	6.233421
5.649241	460.042511	6.238426
5.634133	457.446685	6.243430
5.940202	468.222501	6.248435
5.865913	465.459859	6.253440
5.746621	458.952372	6.258445
6.005646	463.001305	6.263450
5.766273	460.684840	6.268454
6.077552	457.812803	6.273459
6.309371	459.924385	6.278464
6.013524	432.238408	6.283469
5.939573	431.201800	6.288474
5.603579	439.409439	6.293478
5.869876	432.759710	6.298483
5.707909	430.170499	6.303488
5.701446	428.222108	6.308493
5.729240	438.309497	6.313498
5.497200	430.316547	6.318502
5.946201	436.805703	6.323507
5.589748	443.084747	6.328512
5.804117	450.854664	6.333517
5.934496	450.331038	6.338522
5.727135	442.030833	6.343526
5.922010	430.743157	6.348531
5.872815	427.363919	6.353536
5.829820	431.535663	6.358541
5.595302	425.698952	6.363546
5.565992	421.284194	6.368550
5.962932	442.714898	6.373555
5.866713	459.431658	6.378560
6.190003	441.558970	6.383565
6.008930	435.946744	6.388570
5.643017	431.621548	6.393574
5.639367	418.698616	6.398579
5.332684	426.933960	6.403584
5.821685	440.272497	6.408589
5.966202	454.454756	6.413594
5.828077	450.585683	6.418598
5.778701	429.898183	6.423603
5.289808	430.320603	6.428608
5.923348	441.094274	6.433613
6.030682	458.863892	6.438618
5.766770	438.420097	6.443622
5.848415	432.771065	6.448627
5.647495	434.212957	6.453632
5.371121	440.324370	6.458637
5.650869	451.656602	6.463642
5.935282	461.356893	6.468646
6.363133	455.775538	6.473651
5.788017	459.918024	6.478656
5.706033	428.853258	6.483661
5.749382	436.791029	6.488666
5.876240	453.432145	6.493670
5.704600	435.446115	6.498675
5.452638	431.743547	6.503680
5.568187	447.615629	6.508685
5.874998	447.035814	6.513690
5.680890	453.821762	6.518694
6.039888	463.047328	6.523699
5.701313	461.099952	6.528704
5.706878	455.633568	6.533709
5.937880	450.671059	6.538714
5.913039	463.779722	6.543718
6.018775	457.756937	6.548723
5.754985	466.218930	6.553728
5.831748	456.778753	6.558733
5.680148	455.104536	6.563738
5.479056	461.283624	6.568742
5.691912	454.402984	6.573747
5.334119	463.989996	6.578752
5.419275	459.415726	6.583757
5.907426	456.779548	6.588762
5.856193	462.881683	6.593766
6.020276	458.606911	6.598771
5.545984	451.931185	6.603776
5.660522	456.547392	6.608781
5.901106	454.969863	6.613786
5.744997	456.291192	6.618790
5.939263	464.788278	6.623795
5.613135	461.565491	6.628800
5.732922	449.277506	6.633805
5.727294	451.179221	6.638810
5.861506	452.202282	6.643814
5.989519	448.869819	6.648819
5.782058	457.984086	6.653824
5.966537	449.661050	6.658829
6.142598	458.568886	6.663834
5.602338	458.172959	6.668838
6.146386	454.286057	6.673843
6.015137	455.024464	6.678848
5.743945	459.037502	6.683853
5.874955	457.879315	6.688858
6.012522	465.327685	6.693862
6.208614	446.442097	6.698867
5.407815	436.708826	6.703872
5.672473	440.533564	6.708877
5.850709	457.974680	6.713882
5.846607	453.408157	6.718886
5.948216	452.038477	6.723891
5.677195	447.801183	6.728896
5.554301	437.480261	6.733901
5.685679	446.632544	6.738906
5.510190	461.653882	6.743910
5.989141	446.102394	6.748915
5.593290	463.479750	6.753920
5.895597	455.977690	6.758925
5.899741	463.854867	6.763930
5.912225	462.930647	6.768934
5.934218	459.748493	6.773939
6.101987	459.479534	6.778944
5.628791	446.348270	6.783949
5.919004	432.234031	6.788954
5.449759	433.897255	6.793958
5.859037	448.781494	6.798963
5.531503	461.116400	6.803968
5.628736	453.588150	6.808973
5.606372	463.905031	6.813978
5.942940	464.915370	6.818982
5.958767	454.450855	6.823987
5.529437	468.206070	6.828992
5.612216	464.675874	6.833997
6.024078	462.220018	6.839002
5.698452	468.464578	6.844006
5.901502	466.850335	6.849011
5.677933	471.918329	6.854016
5.720583	458.857387	6.859021
5.770724	456.504324	6.864026
5.954907	464.933326	6.869030
5.714590	457.972684	6.874035
5.319313	469.366860	6.879040
5.674732	455.560779	6.884045
5.749939	464.782240	6.889050
5.665347	460.687176	6.894054
5.931806	451.234595	6.899059
5.880562	470.780886	6.904064
5.834160	466.686119	6.909069
5.926753	455.000084	6.914074
5.658133	469.503290	6.919078
5.892434	457.623653	6.924083
5.559192	460.382966	6.929088
5.732217	455.028703	6.934093
5.821660	453.549059	6.939098
6.150914	463.084387	6.944102
5.828385	456.965057	6.949107
5.988676	460.353921	6.954112
5.839929	465.546778	6.959117
5.761472	461.746865	6.964122
5.698192	458.928638	6.969126
5.919542	457.719610	6.974131
6.095735	468.984421	6.979136
6.247380	461.176463	6.984141
5.932697	448.604426	6.989146
5.238161	444.748580	6.994150
5.708165	447.226274	6.999155
5.906752	461.326302	7.004160
5.798638	454.187347	7.009165
5.957542	458.398737	7.014170
5.537194	463.021259	7.019174
5.927075	450.390203	7.024179
5.814308	458.293209	7.029184
5.609535	460.137862	7.034189
5.909958	461.245430	7.039194
5.778791	464.099108	7.044198
6.048103	462.152395	7.049203
5.884951	468.071177	7.054208
5.585290	448.402498	7.059213
5.677873	448.241267	7.064218
5.666956	461.674178	7.069222
5.763611	452.465024	7.074227
5.815183	458.493933	7.079232
5.659590	458.074590	7.084237
5.711367	456.440262	7.089242
5.656564	457.402316	7.094246
5.713345	461.932867	7.099251
5.942635	462.760464	7.104256
5.854233	450.371330	7.109261
5.587639	457.649319	7.114266
5.553904	470.487956	7.119270
5.998580	451.880433	7.124275
6.199111	457.280161	7.129280
5.851285	469.347518	7.134285
5.900575	456.775209	7.139290
5.659990	452.778833	7.144294
6.142171	463.343423	7.149299
6.210739	460.885797	7.154304
5.687940	447.780981	7.159309
5.347949	437.429837	7.164314
5.263738	448.741909	7.169318
5.886662	456.098818	7.174323
5.851996	474.823233	7.179328
5.644598	461.144589	7.184333
5.847401	458.945555	7.189338
5.900238	450.909067	7.194342
5.951947	461.845794	7.199347
5.768837	461.558856	7.204352
5.843353	456.481029	7.209357
5.730432	459.503846	7.214362
5.816289	459.302290	7.219366
6.010792	460.088183	7.224371
6.164942	467.986546	7.229376
5.746767	449.174055	7.234381
5.577081	433.344226	7.239386
5.576459	442.366884	7.244390
5.961322	456.520376	7.249395
5.736349	466.273774	7.254400
5.869904	461.897992	7.259405
6.058032	453.800372	7.264410
5.449655	453.990769	7.269414
5.297988	445.705923	7.274419
5.756175	460.654505	7.279424
5.693423	465.029103	7.284429
5.960313	459.078539	7.289434
5.762526	459.610504	7.294438
5.907828	457.895508	7.299443
5.989984	462.982034	7.304448
5.980466	464.705038	7.309453
6.256926	455.124620	7.314458
5.868410	440.929075	7.319462
5.941602	429.225055	7.324467
5.716094	432.755411	7.329472
5.527153	431.713240	7.334477
5.861236	434.889977	7.339482
5.610307	436.016049	7.344486
5.653556	427.481169	7.349491
5.545489	449.043680	7.354496
5.789664	462.804297	7.359501
6.018507	457.594713	7.364506
5.774302	465.157672	7.369510
5.516959	459.058152	7.374515
5.764025	470.356436	7.379520
5.480504	459.801691	7.384525
5.680521	456.708208	7.389530
5.362588	472.718250	7.394534
5.926599	471.191746	7.399539
5.487252	459.203037	7.404544
5.670525	472.528493	7.409549
6.044768	470.483244	7.414554
5.479194	468.162380	7.419558
5.838668	463.238223	7.424563
5.784692	465.185223	7.429568
5.526865	464.294032	7.434573
5.991579	467.116716	7.439578
5.852612	467.402778	7.444582
6.112343	468.142869	7.449587
5.579541	466.999180	7.454592
5.695123	463.958816	7.459597
6.079152	462.112420	7.464602
5.674582	472.881175	7.469606
6.200722	462.877791	7.474611
6.039114	467.095487	7.479616
5.808558	469.323142	7.484621
5.693404	465.178275	7.489626
5.602431	473.947439	7.494630
6.066019	469.524316	7.499635
6.149658	461.814611	7.504640
6.120407	475.212186	7.509645
6.273307	457.190650	7.514650
5.791817	450.552123	7.519654
5.629462	433.844030	7.524659
5.361414	426.701033	7.529664
5.667731	448.927385	7.534669
5.700248	455.055434	7.539674
5.813480	462.928987	7.544678
6.018516	453.829977	7.549683
6.112149	468.062191	7.554688
5.698176	448.319864	7.559693
5.687496	431.342337	7.564698
5.707356	439.063692	7.569702
5.777489	459.170303	7.574707
6.058529	457.996299	7.579712
5.689091	447.502326	7.584717
5.565023	432.567464	7.589722
5.320464	453.133718	7.594726
5.723242	459.324787	7.599731
6.051220	466.636326	7.604736
5.832214	474.061249	7.609741
6.134404	469.294838	7.614746
5.891673	462.474784	7.619750
5.467489	445.736548	7.624755
6.018888	460.760883	7.629760
5.447934	469.147557	7.634765
5.796150	463.378496	7.639770
6.048648	467.086272	7.644774
6.053950	471.930180	7.649779
5.992226	447.572716	7.654784
5.675518	436.469222	7.659789
5.579846	430.620613	7.664794
5.405818	445.026180	7.669798
5.583849	452.545401	7.674803
5.690698	463.377616	7.679808
6.063627	469.397423	7.684813
6.005297	460.358211	7.689818
5.788717	461.549936	7.694822
6.068952	451.365221	7.699827
5.290048	440.747923	7.704832
5.601331	458.009498	7.709837
5.997111	462.654503	7.714842
5.981219	464.763516	7.719846
6.109258	462.031071	7.724851
5.900815	445.460216	7.729856
5.579548	438.067924	7.734861
5.556055	438.585193	7.739866
5.700373	451.788816	7.744870
5.836222	449.692302	7.749875
5.999368	463.142324	7.754880
5.652739	462.207010	7.759885
6.024523	468.684079	7.764890
5.800004	471.674335	7.769894
5.956014	444.145209	7.774899
5.912581	435.872671	7.779904
5.702729	440.616671	7.784909
5.901388	435.744750	7.789914
5.734257	434.265875	7.794918
5.824446	434.213857	7.799923
6.187931	439.518577	7.804928
5.437411	434.167778	7.809933
5.847201	430.694043	7.814938
5.670290	440.515447	7.819942
5.536340	431.281670	7.824947
5.575185	441.249143	7.829952
5.642952	459.504374	7.834957
5.857085	451.647519	7.839962
5.815914	468.719923	7.844966
6.091286	470.699016	7.849971
5.924744	450.423601	7.854976
5.354179	452.468400	7.859981
5.906171	453.805895	7.864986
5.451531	463.711687	7.869990
5.777726	461.255783	7.874995
5.927267	470.701836	7.880000
5.714391	478.430299	7.885005
5.735783	464.648828	7.890010
5.853437	465.504050	7.895014
6.030897	467.814628	7.900019
5.959238	474.495604	7.905024
5.786982	452.008373	7.910029
5.980865	446.699600	7.915034
5.654840	442.681436	7.920038
5.789150	425.971285	7.925043
5.706017	442.364344	7.930048
5.666970	454.299664	7.935053
5.899322	455.603757	7.940058
5.388179	478.548795	7.945062
5.852367	460.107726	7.950067
5.733476	459.388027	7.955072
5.681421	471.531405	7.960077
5.719526	472.070262	7.965082
5.538314	466.349625	7.970086
5.589386	460.987496	7.975091
5.735509	466.022115	7.980096
5.717494	473.904242	7.985101
5.782381	468.710700	7.990106
5.644901	468.662270	7.995110
5.698623	462.801094	8.000115
5.717195	449.278486	8.005133
5.857900	466.731236	8.010150
5.698854	463.541350	8.015168
5.760527	462.026733	8.020186
5.837426	465.504410	8.025203
5.651256	460.042126	8.030221
5.584679	462.156405	8.035238
5.959580	455.445347	8.040256
5.824774	465.590463	8.045274
5.954159	463.842852	8.050291
6.008661	462.033026	8.055309
5.723729	464.628768	8.060326
6.088984	448.935481	8.065344
5.900360	466.962427	8.070362
5.816907	459.568515	8.075379
5.832001	458.474796	8.080397
5.907412	464.206374	8.085414
5.723939	453.702786	8.090432
5.788826	459.754932	8.095450
5.692280	464.864475	8.100467
5.994125	454.366983	8.105485
5.716450	454.894640	8.110502
6.170446	458.126669	8.115520
5.803493	463.821927	8.120538
5.994650	462.867973	8.125555
5.930348	455.156890	8.130573
5.995789	456.863310	8.135590
6.140928	456.117215	8.140608
6.051920	457.779588	8.145626
5.897569	464.694465	8.150643
6.110392	451.640380	8.155661
5.706861	454.083611	8.160678
5.998225	456.595529	8.165696
6.022187	453.864176	8.170714
5.925544	455.293608	8.175731
6.134782	456.282908	8.180749
5.988081	457.665112	8.185766
6.104057	447.853124	8.190784
6.081474	453.782646	8.195802
5.720211	465.524894	8.200819
5.815291	450.064699	8.205837
5.721210	463.239446	8.210854
5.939914	461.683232	8.215872
6.117352	454.410543	8.220890
5.809109	463.627141	8.225907
5.925663	461.230805	8.230925
6.062083	452.331481	8.235942
5.913914	460.402176	8.240960
5.910627	467.387246	8.245978
6.022420	447.970403	8.250995
5.902894	455.691356	8.256013
6.110488	466.505620	8.261030
6.010155	468.423847	8.266048
6.004085	473.886573	8.271066
6.318688	474.352859	8.276083
6.060605	470.387380	8.281101
5.798030	468.126615	8.286118
6.243761	476.547698	8.291136
6.311881	480.889343	8.296154
5.928336	470.906696	8.301171
6.422195	469.225892	8.306189
6.151293	472.247081	8.311206
6.244312	460.866572	8.316224
5.994263	451.425733	8.321242
6.089379	453.130989	8.326259
6.315239	453.488049	8.331277
5.968626	450.685977	8.336294
5.931985	458.143484	8.341312
6.168833	455.883141	8.346330
6.131192	456.246256	8.351347
6.103331	449.126467	8.356365
6.208058	473.259836	8.361382
6.362843	471.611155	8.366400
6.257760	467.652963	8.371418
6.071856	464.976857	8.376435
6.034573	454.913479	8.381453
6.088414	467.178735	8.386470
6.111801	472.972250	8.391488
6.334018	476.936042	8.396506
6.121854	486.303866	8.401523
6.454268	474.771801	8.406541
6.028215	481.681302	8.411558
5.730818	476.695467	8.416576
6.012886	484.683167	8.421594
6.041025	487.739863	8.426611
6.085558	482.859493	8.431629
6.153449	490.736460	8.436646
6.101482	494.631124	8.441664
6.235073	496.076043	8.446682
6.077612	489.208708	8.451699
5.990934	487.976130	8.456717
6.162700	491.530438	8.461734
6.124931	487.305069	8.466752
6.427160	482.284495	8.471770
6.414835	482.556239	8.476787
6.655639	480.999225	8.481805
6.466953	496.567383	8.486822
6.354909	485.937819	8.491840
6.691832	490.532817	8.496858
6.356882	490.466327	8.501875
6.674465	492.796396	8.506893
6.490851	490.476427	8.511910
6.245297	491.123258	8.516928
6.246627	488.881659	8.521946
6.325183	496.863636	8.526963
6.300108	498.278096	8.531981
6.611855	482.981823	8.536998
6.539700	487.487371	8.542016
6.638791	487.635115	8.547034
6.315614	489.821619	8.552051
6.446375	484.394532	8.557069
6.266356	477.903784	8.562087
6.224332	478.211730	8.567104
6.485669	486.678937	8.572122
6.276794	499.674402	8.577139
6.467945	488.525733	8.582157
6.541799	490.876990	8.587175
6.713977	492.532809	8.592192
6.759205	467.465925	8.597210
6.491850	464.474215	8.602227
6.485184	464.462013	8.607245
6.418403	454.766327	8.612263
6.491135	460.413128	8.617280
6.217815	454.978928	8.622298
6.344996	455.294926	8.627315
6.463332	452.431564	8.632333
6.324536	456.823536	8.637351
6.200606	458.781481	8.642368
6.639575	472.985429	8.647386
6.599928	486.910981	8.652403
6.670254	469.097282	8.657421
6.576347	463.193758	8.662439
6.431331	459.790084	8.667456
6.592812	450.229574	8.672474
6.214695	445.733169	8.677491
6.461919	463.466083	8.682509
6.418920	485.341001	8.687527
6.661630	486.636418	8.692544
6.582980	471.965382	8.697562
6.223907	474.966307	8.702579
6.837844	482.680310	8.707597
6.764565	494.309943	8.712615
6.644567	470.220554	8.717632
6.679808	464.111276	8.722650
6.270048	458.131829	8.727667
6.507070	461.029223	8.732685
6.575030	463.064489	8.737703
6.500387	478.036837	8.742720
6.756446	478.557080	8.747738
6.386231	472.292509	8.752755
6.647379	489.336880	8.757773
6.536828	482.184688	8.762791
6.752799	492.423592	8.767808
6.736676	488.245816	8.772826
6.541131	481.042724	8.777843
6.410767	477.123543	8.782861
6.372685	475.285816	8.787879
6.444181	492.689416	8.792896
6.661405	486.999370	8.797914
6.323469	493.371688	8.802931
6.736528	488.795692	8.807949
6.627196	493.189792	8.812967
6.537348	486.556016	8.817984
6.995677	489.921756	8.823002
6.760428	487.391764	8.828019
6.579091	479.709062	8.833037
6.603651	485.319257	8.838055
6.803851	500.001867	8.843072
6.933433	486.795205	8.848090
6.789278	489.103865	8.853107
6.726228	487.466284	8.858125
6.809373	485.946050	8.863143
6.440102	491.642587	8.868160
6.635171	493.054221	8.873178
6.647786	492.209283	8.878195
6.616040	470.247478	8.883213
6.359869	491.764901	8.888231
6.576407	497.637604	8.893248
6.543496	481.904889	8.898266
6.696347	481.593745	8.903283
6.771943	488.639888	8.908301
6.597873	487.165605	8.913319
6.611543	483.764534	8.918336
7.119966	499.881230	8.923354
6.738459	501.475434	8.928371
6.974903	481.971525	8.933389
6.944278	487.648702	8.938407
6.931882	488.664988	8.943424
6.954963	482.804609	8.948442
6.922830	489.171655	8.953459
7.169671	481.019457	8.958477
6.896252	481.794490	8.963495
6.835067	493.594134	8.968512
6.951326	481.442017	8.973530
6.797528	484.328920	8.978547
6.816449	498.164604	8.983565
7.163701	489.024653	8.988583
6.820966	488.315786	8.993600
6.998286	492.065985	8.998618
7.207928	495.632633	9.003635
6.973460	482.671236	9.008653
6.525935	488.948596	9.013671
6.665090	492.488416	9.018688
6.762540	482.047021	9.023706
6.500230	483.529223	9.028723
6.577971	480.629759	9.033741
6.925419	496.064246	9.038759
6.635180	493.942272	9.043776
6.730677	501.129787	9.048794
7.200532	520.835595	9.053811
7.282653	521.184823	9.058829
7.412353	506.523998	9.063847
6.905234	510.299928	9.068864
7.040570	494.114682	9.073882
6.854278	473.849126	9.078899
6.920390	487.293814	9.083917
7.022720	492.738239	9.088935
6.635207	490.678099	9.093952
6.843948	506.133059	9.098970
7.058399	515.805813	9.103987
7.161931	528.357629	9.109005
7.092745	521.668564	9.114023
6.945183	531.689086	9.119040
6.677737	526.602439	9.124058
6.942493	520.961305	9.129075
6.922653	523.371939	9.134093
7.125142	534.587503	9.139111
6.899868	534.481436	9.144128
6.807552	522.659659	9.149146
6.664044	520.797133	9.154163
6.657418	535.393805	9.159181
7.011320	526.700082	9.164199
6.803827	524.207909	9.169216
6.406695	518.546167	9.174234
6.815325	549.381769	9.179251
6.801732	557.313370	9.184269
7.084342	545.669133	9.189287
7.287505	558.095672	9.194304
7.049630	562.732741	9.199322
7.460738	550.592854	9.204339
7.092427	559.297299	9.209357
7.003984	561.058683	9.214375
6.995301	551.985291	9.219392
7.173754	548.598303	9.224410
7.110023	555.646738	9.229427
7.236793	554.992829	9.234445
7.326227	555.741259	9.239463
7.180621	554.187675	9.244480
7.345627	554.593763	9.249498
7.459497	551.162144	9.254515
7.003893	561.070141	9.259533
7.250388	548.340165	9.264551
6.900485	553.390053	9.269568
7.168940	554.262411	9.274586
7.415077	554.512108	9.279603
7.186476	554.663231	9.284621
7.583110	558.077067	9.289639
7.165332	555.314684	9.294656
7.134205	556.650244	9.299674
7.500516	556.581325	9.304691
7.214818	551.723328	9.309709
7.674195	553.824209	9.314727
7.455844	553.113578	9.319744
7.373140	549.048637	9.324762
7.467044	550.996278	9.329779
7.510744	566.190739	9.334797
7.479330	558.714277	9.339815
7.686870	550.479579	9.344832
7.452718	545.009155	9.349850
7.172635	539.297950	9.354867
7.141793	531.272012	9.359885
7.489138	543.357160	9.364903
7.425646	550.044013	9.369920
7.554263	531.922048	9.374938
7.418900	531.749755	9.379955
7.197295	530.229988	9.384973
7.382212	519.600231	9.389991
7.345644	524.396599	9.395008
7.310659	521.053550	9.400026
7.495276	526.503970	9.405043
6.938299	534.710556	9.410061
7.440202	541.254766	9.415079
7.519370	549.587188	9.420096
7.321503	546.858232	9.425114
7.590190	555.033674	9.430131
7.505883	568.065389	9.435149
7.615313	546.809720	9.440167
7.413384	553.104085	9.445184
7.426201	558.330893	9.450202
7.452384	548.726652	9.455219
7.171839	556.470625	9.460237
7.282557	546.017646	9.465255
7.293739	550.212749	9.470272
7.254167	554.139427	9.475290
7.468646	546.870414	9.480307
7.331683	551.672655	9.485325
7.327684	558.143621	9.490343
7.221412	548.970141	9.495360
7.200198	561.433764	9.500378
7.330204	552.688167	9.505395
7.097481	560.041541	9.510413
7.575648	578.953005	9.515431
7.643544	586.186844	9.520448
7.600629	582.105282	9.525466
7.872290	586.093503	9.530483
7.687342	575.270258	9.535501
7.305052	563.062897	9.540519
7.467947	576.233257	9.545536
7.231262	578.428113	9.550554
7.792563	578.843400	9.555571
7.766759	589.970380	9.560589
7.696479	595.142935	9.565607
7.438944	592.257331	9.570624
7.891851	589.174612	9.575642
7.872352	576.079501	9.580659
8.027078	585.684232	9.585677
7.967154	568.788315	9.590695
7.699941	551.546634	9.595712
7.191165	555.600252	9.600730
7.478128	556.811410	9.605747
7.274564	560.163838	9.610765
7.771726	574.848812	9.615783
7.993737	593.478578	9.620800
7.864441	583.793436	9.625818
8.108782	561.255078	9.630835
7.680995	565.046646	9.635853
7.797080	562.405047	9.640871
7.732481	544.939771	9.645888
7.701304	553.684640	9.650906
7.929797	555.476996	9.655923
7.631681	558.591755	9.660941
7.781766	560.239523	9.665959
8.018000	551.579796	9.670976
7.489827	552.494353	9.675994
7.956178	552.319943	9.681011
7.542913	561.532305	9.686029
7.657457	548.789792	9.691047
7.738894	562.930886	9.696064
7.689282	575.054007	9.701082
7.979145	566.452029	9.706099
7.868206	564.668056	9.711117
7.990962	564.994530	9.716135
7.607281	550.110398	9.721152
7.186111	557.908805	9.726170
7.892571	573.083097	9.731187
7.652229	583.370705	9.736205
8.011748	576.055174	9.741223
7.899332	596.279659	9.746240
7.700621	599.612302	9.751258
7.969843	590.715750	9.756275
7.849801	589.969387	9.761293
7.893898	601.055006	9.766311
7.679125	593.646912	9.771328
7.651045	588.452689	9.776346
7.920679	589.454846	9.781363
7.793637	596.762925	9.786381
7.869853	593.304061	9.791399
8.088947	598.815135	9.796416
7.751041	597.164316	9.801434
7.900155	592.950545	9.806451
7.957073	599.597840	9.811469
7.965936	600.293065	9.816487
7.897192	582.090491	9.821504
7.513435	588.049148	9.826522
7.885065	595.229254	9.831539
7.919823	595.911344	9.836557
7.907709	594.905165	9.841575
8.165520	602.660468	9.846592
7.839554	612.575611	9.851610
8.156983	612.591723	9.856627
8.116395	600.199837	9.861645
7.774648	599.904398	9.866663
8.178335	606.026964	9.871680
8.262049	611.297082	9.876698
8.158021	599.043116	9.881715
7.936408	600.402680	9.886733
8.026802	596.509770	9.891751
8.468173	605.804696	9.896768
8.013199	605.505335	9.901786
8.176195	599.072689	9.906803
8.022440	589.456730	9.911821
7.738971	593.019279	9.916839
8.175447	602.395213	9.921856
7.926962	617.047873	9.926874
8.288345	617.750184	9.931891
8.289045	632.088112	9.936909
8.221396	625.301523	9.941927
8.349719	618.787608	9.946944
8.134054	613.049493	9.951962
8.148138	595.629609	9.956979
7.670109	599.012052	9.961997
7.606878	620.289938	9.967015
8.212965	615.032431	9.972032
8.086083	620.503759	9.977050
8.328686	621.645004	9.982067
8.161559	619.534157	9.987085
8.266011	619.531637	9.992103
8.409090	627.013157	9.997120
8.324411	622.114439	10.002138
8.299582	617.414844	10.007155
8.467805	628.572374	10.012173
8.210744	626.880342	10.017191
8.389771	613.377958	10.022208
8.211154	630.589040	10.027226
8.512650	619.031175	10.032243
8.269076	617.313102	10.037261
8.336597	615.548144	10.042279
8.216599	616.330007	10.047296
8.080378	629.255219	10.052314
8.070019	619.213755	10.057331
8.055789	623.646003	10.062349
8.242669	630.770947	10.067367
8.312282	616.908961	10.072384
8.289669	619.693123	10.077402
8.198468	617.978997	10.082419
8.241382	620.015175	10.087437
8.151392	636.875464	10.092455
8.020291	618.445798	10.097472
8.019418	621.773895	10.102490
8.317092	639.923000	10.107507
8.385386	661.541241	10.112525
8.511671	655.246108	10.117543
8.855718	654.793346	10.122560
8.566773	661.229375	10.127578
8.435149	640.403689	10.132595
8.388480	622.555910	10.137613
8.477275	623.317832	10.142631
8.647109	624.700290	10.147648
8.375731	628.437881	10.152666
8.337836	634.605881	10.157683
8.565799	641.028805	10.162701
8.510949	641.635762	10.167719
8.953475	631.963354	10.172736
8.440221	645.665311	10.177754
8.347591	627.940157	10.182771
8.510059	619.436451	10.187789
8.280211	645.710001	10.192807
8.512355	640.697022	10.197824
8.721522	663.481315	10.202842
8.586987	646.426909	10.207859
8.829617	647.210743	10.212877
8.732601	648.884202	10.217895
8.526447	635.113237	10.222912
8.557666	641.157340	10.227930
8.421922	631.037494	10.232947
8.587242	626.504170	10.237965
8.278704	649.235343	10.242983
8.878549	649.930426	10.248000
8.853708	658.322409	10.253018
8.659117	643.612703	10.258035
8.771146	632.448961	10.263053
8.357001	631.830612	10.268071
8.768461	644.993018	10.273088
8.609207	632.546125	10.278106
8.311774	639.407576	10.283123
8.592670	647.264478	10.288141
8.528127	666.703347	10.293159
8.744234	659.838951	10.298176
8.776269	665.603358	10.303194
8.609771	652.016731	10.308211
8.835985	662.045731	10.313229
8.408741	664.054713	10.318247
8.806733	645.964263	10.323264
8.604304	660.987527	10.328282
8.254786	658.753500	10.333299
8.413141	658.395783	10.338317
8.383954	661.893200	10.343335
8.551067	660.382985	10.348352
8.726291	665.399070	10.353370
8.935338	676.566420	10.358387
9.301931	669.698012	10.363405
8.809345	674.723694	10.368423
9.097528	662.612202	10.373440
8.635138	666.530551	10.378458
8.532629	669.513027	10.383475
8.884433	659.540104	10.388493
8.994891	667.978125	10.393511
8.996081	657.018964	10.398528
8.908412	661.432559	10.403546
8.666215	659.220946	10.408563
8.825904	666.089428	10.413581
8.763822	652.463403	10.418599
8.855245	655.301546	10.423616
9.031496	661.312242	10.428634
8.842767	667.695105	10.433651
8.839228	660.713396	10.438669
8.472665	660.068386	10.443687
8.976678	677.134136	10.448704
9.146312	677.227221	10.453722
9.114053	688.887617	10.458739
8.796848	681.698926	10.463757
9.230518	688.953847	10.468775
8.996699	670.540305	10.473792
9.097377	680.401715	10.478810
8.796069	667.942055	10.483827
9.362895	665.733232	10.488845
8.978549	679.912833	10.493863
9.188363	662.814886	10.498880
9.104287	655.723973	10.503898
8.858377	661.051928	10.508915
9.012700	652.773028	10.513933
8.884298	662.140795	10.518951
8.925190	665.647789	10.523968
9.252720	667.900863	10.528986
8.950082	676.268994	10.534003
9.217230	689.012166	10.539021
9.243949	680.190573	10.544039
9.022666	668.930637	10.549056
9.213564	666.781577	10.554074
8.899638	683.005337	10.559091
9.175339	671.628433	10.564109
9.207646	694.201200	10.569127
9.162968	690.875657	10.574144
9.089246	680.215220	10.579162
9.101468	692.084464	10.584179
9.303983	686.044286	10.589197
9.130584	689.607955	10.594215
9.435320	690.363717	10.599232
9.309165	674.005298	10.604250
9.053409	673.203618	10.609267
9.095526	668.156298	10.614285
8.987448	683.083397	10.619303
9.271277	683.308368	10.624320
9.508759	690.298525	10.629338
9.362591	698.522921	10.634355
9.544897	681.010684	10.639373
9.164746	681.181341	10.644391
9.455712	672.824938	10.649408
9.199168	664.926567	10.654426
9.216716	659.158159	10.659443
9.137937	667.959474	10.664461
9.403825	674.002498	10.669479
9.288856	675.453282	10.674496
9.459693	674.998836	10.679514
9.182110	679.206958	10.684531
9.332325	671.093557	10.689549
9.432486	680.783236	10.694567
9.674861	690.882897	10.699584
9.473111	673.625930	10.704602
9.265492	673.551188	10.709619
9.510226	668.278592	10.714637
9.172052	664.477941	10.719655
9.019508	660.361041	10.724672
9.252677	675.797866	10.729690
9.181402	685.028573	10.734707
9.474738	687.111744	10.739725
9.355666	705.941883	10.744743
8.957603	696.261330	10.749760
9.214598	690.904925	10.754778
9.296067	696.388984	10.759795
9.542464	693.697880	10.764813
9.122191	696.303825	10.769831
9.254942	700.301650	10.774848
9.692284	699.761732	10.779866
9.359616	699.418736	10.784883
9.238105	704.723195	10.789901
9.261149	702.426904	10.794919
9.338810	716.869787	10.799936
9.587916	726.017855	10.804954
9.617396	731.189419	10.809971
9.640665	726.638702	10.814989
9.763388	743.599559	10.820007
9.417335	724.631284	10.825024
9.464974	722.379440	10.830042
9.593823	733.247153	10.835059
9.723559	730.971506	10.840077
9.580625	724.090741	10.845095
9.752711	722.064051	10.850112
9.347062	722.600564	10.855130
9.346454	733.179889	10.860147
9.655350	725.081567	10.865165
9.509104	729.596674	10.870183
9.008066	731.803257	10.875200
9.588587	727.660155	10.880218
9.199573	729.140782	10.885235
9.575127	727.191862	10.890253
9.606928	726.295324	10.895271
9.523587	734.354563	10.900288
9.588911	738.152656	10.905306
9.786736	747.829878	10.910323
9.859962	747.308900	10.915341
9.828174	737.846379	10.920359
9.481538	739.851397	10.925376
9.882615	744.195071	10.930394
9.746661	766.279708	10.935411
9.874259	754.169883	10.940429
9.892846	762.134748	10.945447
9.826215	748.702562	10.950464
9.943702	744.896162	10.955482
9.764289	726.001804	10.960499
9.649823	723.182080	10.965517
9.777773	732.860902	10.970535
9.606028	751.775278	10.975552
9.869966	754.077744	10.980570
9.707422	767.342003	10.985587
9.919832	753.964761	10.990605
10.010650	763.141568	10.995623
9.721153	764.353636	11.000640
9.999345	755.900402	11.005658
9.812114	757.780280	11.010675
10.022321	763.685227	11.015693
10.273635	761.198477	11.020711
10.073119	760.884418	11.025728
10.063397	761.357569	11.030746
9.893280	767.280890	11.035763
9.851904	756.401907	11.040781
10.175078	764.938168	11.045799
9.561256	757.536503	11.050816
9.887098	762.348433	11.055834
9.731480	763.843928	11.060851
9.890363	754.077301	11.065869
9.893985	762.075637	11.070887
9.657535	768.055089	11.075904
10.309320	759.577507	11.080922
9.981985	761.037711	11.085939
10.199674	770.593872	11.090957
9.877870	759.847926	11.095975
10.046208	768.282046	11.100992
10.136171	755.795147	11.106010
9.943881	767.571991	11.111027
9.709148	757.238840	11.116045
10.231238	764.778240	11.121063
9.897444	770.922964	11.126080
10.192889	755.463202	11.131098
9.875465	775.071041	11.136115
10.338299	772.262282	11.141133
10.186119	769.505072	11.146151
9.860196	773.608729	11.151168
10.291423	767.030721	11.156186
10.164154	769.897153	11.161203
10.265115	762.112452	11.166221
10.277035	763.915530	11.171239
9.991936	764.840312	11.176256
10.408988	767.301497	11.181274
10.201580	756.702069	11.186291
9.823065	770.654652	11.191309
10.110697	786.804891	11.196327
10.071892	795.945374	11.201344
10.541677	805.247141	11.206362
10.795925	817.132282	11.211379
10.433879	792.097830	11.216397
10.582294	772.364053	11.221415
10.182953	781.835712	11.226432
10.305018	768.541878	11.231450
10.369566	767.457875	11.236467
10.473537	771.375057	11.241485
10.324715	760.659075	11.246503
10.354113	763.404753	11.251520
10.535752	768.269840	11.256538
10.256920	764.481006	11.261555
10.496130	761.203004	11.266573
10.456062	755.675238	11.271591
10.316767	765.601552	11.276608
10.400401	758.876993	11.281626
10.246976	765.659003	11.286643
10.160706	770.183597	11.291661
10.697677	783.878917	11.296679
10.128953	778.618395	11.301696
10.725579	785.474947	11.306714
10.183679	801.117530	11.311731
10.440964	803.297209	11.316749
10.734535	798.968876	11.321767
10.503628	807.071827	11.326784
10.390791	804.972746	11.331802
10.618796	808.148416	11.336819
10.315942	809.187236	11.341837
10.754669	803.363440	11.346855
10.699546	800.876547	11.351872
10.921792	792.686525	11.356890
10.674715	779.689075	11.361907
10.209758	764.212081	11.366925
10.770138	774.965703	11.371943
10.600192	790.835137	11.376960
10.679704	779.514586	11.381978
10.861144	771.287430	11.386995
10.289314	774.558468	11.392013
10.546302	782.928448	11.397031
10.332632	795.847508	11.402048
10.475478	798.263577	11.407066
10.962546	794.455526	11.412083
10.599022	794.939124	11.417101
10.853033	792.194688	11.422119
10.866515	799.922371	11.427136
10.544912	799.710688	11.432154
10.929878	797.536624	11.437171
10.484732	804.976785	11.442189
11.021326	798.836284	11.447207
10.748522	801.539407	11.452224
11.033926	800.338898	11.457242
10.656009	793.930022	11.462259
10.588809	799.854750	11.467277
10.686559	783.223627	11.472295
10.615480	797.257293	11.477312
10.623631	791.059467	11.482330
10.988829	797.470701	11.487347
10.586157	799.551215	11.492365
10.918132	787.419791	11.497383
10.718054	801.110576	11.502400
10.645069	795.071602	11.507418
10.685359	802.998262	11.512435
10.503743	798.920178	11.517453
10.450010	789.861667	11.522471
10.762127	810.369555	11.527488
10.852601	805.080976	11.532506
10.776316	795.114256	11.537523
10.770465	802.796817	11.542541
11.019019	813.741736	11.547559
10.844026	812.064856	11.552576
11.083218	822.206755	11.557594
11.063376	818.879737	11.562611
10.808341	821.445700	11.567629
11.161557	827.517062	11.572647
10.653206	833.143221	11.577664
10.973387	827.721219	11.582682
10.979113	826.790901	11.587699
10.962958	822.979702	11.592717
11.055177	813.133422	11.597735
11.035657	824.942771	11.602752
10.870886	821.491306	11.607770
10.878904	819.958361	11.612787
10.750169	827.915033	11.617805
11.181318	822.415552	11.622823
10.983052	822.516494	11.627840
10.777608	814.361123	11.632858
10.939394	817.737171	11.637875
10.814023	820.597592	11.642893
11.042499	816.682593	11.647911
11.080475	830.346857	11.652928
11.200028	852.112082	11.657946
11.504383	848.029447	11.662963
11.056604	840.004546	11.667981
11.080635	834.938020	11.672999
11.189376	844.702748	11.678016
11.310848	845.384492	11.683034
11.335209	848.426533	11.688051
11.087212	857.868601	11.693069
11.316418	850.932874	11.698087
11.402041	853.314913	11.703104
11.206062	860.154971	11.708122
11.504296	847.170083	11.713139
11.292808	837.327825	11.718157
11.467372	843.667059	11.723175
11.251818	825.955791	11.728192
11.171691	813.518210	11.733210
11.288883	838.859805	11.738227
11.274202	843.019407	11.743245
11.478121	850.482814	11.748263
11.180377	855.893600	11.753280
11.166776	842.791973	11.758298
11.293161	851.016478	11.763315
11.239142	865.669908	11.768333
11.132248	855.202593	11.773351
11.337376	857.007112	11.778368
10.932041	863.759353	11.783386
11.564610	853.472535	11.788403
11.355333	857.500650	11.793421
11.340797	846.133596	11.798439
11.154159	856.360749	11.803456
11.102693	864.912531	11.808474
11.393149	856.696934	11.813491
11.395913	881.301646	11.818509
11.508472	880.818052	11.823527
11.775397	881.149837	11.828544
11.509541	886.397617	11.833562
11.516258	885.241386	11.838579
11.699156	888.839608	11.843597
11.784828	886.043561	11.848615
11.688787	873.802226	11.853632
11.576077	865.450238	11.858650
11.971418	855.850534	11.863667
11.444182	862.662282	11.868685
11.503879	851.389433	11.873703
11.224022	859.355449	11.878720
11.301782	875.244063	11.883738
11.906426	878.569079	11.888755
11.474459	884.533947	11.893773
11.847255	886.132940	11.898791
12.176331	890.516600	11.903808
11.635146	884.978115	11.908826
12.087555	868.953423	11.913843
11.814946	860.197332	11.918861
11.765171	867.781200	11.923879
11.587903	859.983680	11.928896
11.386956	855.536403	11.933914
11.602790	867.907566	11.938931
11.893642	887.791531	11.943949
11.800692	881.389846	11.948967
12.207120	882.736180	11.953984
11.937666	872.706566	11.959002
12.042251	851.459642	11.964019
11.653658	851.338049	11.969037
11.773827	861.009971	11.974055
11.612948	861.862960	11.979072
11.736570	871.723752	11.984090
11.886062	883.523617	11.989107
11.757400	887.543632	11.994125
11.792953	886.065863	11.999143
12.133227	895.804858	12.004160
11.952123	890.309307	12.009178
12.099564	879.069271	12.014195
12.008289	887.668581	12.019213
11.865216	892.793729	12.024231
11.911206	874.227719	12.029248
11.652499	880.442542	12.034266
11.838595	884.933771	12.039283
11.683391	889.944704	12.044301
11.856279	889.257475	12.049319
12.124240	889.933021	12.054336
11.563720	888.816997	12.059354
12.028034	878.032967	12.064371
12.240216	886.052206	12.069389
12.065192	888.565595	12.074407
12.318854	884.758995	12.079424
12.138691	882.941453	12.084442
11.876437	877.947513	12.089459
12.181497	890.656443	12.094477
12.198786	890.063617	12.099495
12.269051	882.550611	12.104512
11.991348	892.035792	12.109530
12.014125	903.537380	12.114547
11.986320	895.691819	12.119565
12.233697	895.348514	12.124583
12.286958	897.972774	12.129600
12.166884	903.968571	12.134618
12.129724	890.844620	12.139635
11.929182	891.523195	12.144653
11.938873	894.470344	12.149671
12.274199	915.215634	12.154688
12.120121	916.287344	12.159706
12.336754	919.793793	12.164723
12.594734	926.666420	12.169741
12.256920	911.468704	12.174759
12.502196	910.482556	12.179776
12.317821	906.436783	12.184794
12.426869	894.053291	12.189811
12.264410	892.197690	12.194829
12.115550	902.265214	12.199847
12.391787	909.218364	12.204864
12.486887	925.302847	12.209882
12.398254	926.389919	12.214899
12.318430	920.189949	12.219917
12.366849	917.714956	12.224935
12.895608	921.859463	12.229952
12.431995	911.351963	12.234970
12.218102	896.224023	12.239987
12.297555	908.591777	12.245005
12.183655	917.030503	12.250023
12.512648	919.946539	12.255040
12.334310	929.712905	12.260058
12.618568	921.643646	12.265075
12.958510	918.812166	12.270093
12.527402	927.298103	12.275111
12.887848	923.057879	12.280128
12.147979	930.274709	12.285146
12.790225	922.232887	12.290163
12.761080	925.667279	12.295181
12.494182	924.200618	12.300199
12.730712	923.392063	12.305216
12.410106	928.998252	12.310234
12.539983	932.572182	12.315251
12.586480	915.788588	12.320269
12.448750	922.384544	12.325287
12.648335	921.428088	12.330304
12.354649	933.125081	12.335322
12.663568	921.491761	12.340339
12.628415	925.737431	12.345357
12.309533	937.662370	12.350375
12.766239	925.652522	12.355392
12.616014	929.815260	12.360410
12.432019	929.338751	12.365427
12.413212	931.776143	12.370445
12.447608	935.241367	12.375463
12.855865	945.297742	12.380480
12.584317	958.212135	12.385498
12.749180	960.436436	12.390515
13.063936	952.078412	12.395533
12.761692	958.564095	12.400551
13.183159	965.509015	12.405568
12.691267	951.926988	12.410586
12.693360	953.312693	12.415603
12.806423	951.109737	12.420621
12.450267	949.354828	12.425639
12.641990	953.293572	12.430656
12.693240	960.878505	12.435674
12.768447	956.082073	12.440691
12.723643	962.832245	12.445709
12.375711	962.647249	12.450727
12.721005	960.317150	12.455744
12.833118	979.962414	12.460762
13.163169	983.190732	12.465779
13.053359	980.010216	12.470797
12.760708	986.629932	12.475815
13.090564	989.833780	12.480832
13.387088	992.838154	12.485850
13.051730	978.700899	12.490867
13.013179	967.685793	12.495885
12.737115	978.193505	12.500903
13.339105	979.488341	12.505920
13.013754	988.456253	12.510938
13.129417	997.622304	12.515955
12.900254	985.539076	12.520973
13.346965	986.763134	12.525991
13.293372	990.565492	12.531008
13.355789	982.187353	12.536026
13.052759	979.658934	12.541043
13.325754	972.711389	12.546061
13.211936	981.343802	12.551079
13.012243	967.658561	12.556096
13.293976	980.637220	12.561114
13.286747	989.768565	12.566131
13.591580	977.313190	12.571149
12.928081	982.338776	12.576167
13.043917	980.400271	12.581184
13.205087	977.696239	12.586202
13.341440	978.793763	12.591219
13.418631	989.485975	12.596237
13.193246	984.434540	12.601255
13.752187	988.454512	12.606272
13.430929	981.653781	12.611290
13.259883	981.646406	12.616307
13.268766	968.278405	12.621325
13.356620	988.646557	12.626343
13.433396	980.196766	12.631360
13.105869	977.156051	12.636378
13.212389	991.244584	12.641395
13.512354	985.208949	12.646413
13.480878	986.751949	12.651431
13.154365	980.260399	12.656448
13.087628	986.120370	12.661466
12.979836	984.666477	12.666483
13.551885	980.306146	12.671501
13.066861	982.784870	12.676519
13.414342	986.391245	12.681536
13.238832	1003.989365	12.686554
13.262707	1006.811576	12.691571
13.279604	1002.668845	12.696589
13.190607	1013.236005	12.701607
13.624699	1013.490176	12.706624
13.753662	1017.811685	12.711642
13.771862	1017.116063	12.716659
13.847563	1015.717262	12.721677
13.498229	1020.841899	12.726695
13.640461	1015.262362	12.731712
13.894924	1012.797292	12.736730
13.706951	1016.431051	12.741747
13.843073	1014.690236	12.746765
13.911527	1019.168668	12.751783
13.808088	1018.772036	12.756800
13.931479	1018.142579	12.761818
13.886882	1018.837310	12.766835
14.160539	1018.542308	12.771853
13.839490	1020.352320	12.776871
13.765280	1009.471499	12.781888
13.962394	1002.694327	12.786906
13.396668	994.787638	12.791923
13.780977	1010.201397	12.796941
13.441901	1019.554402	12.801959
13.838152	1013.047412	12.806976
14.293325	1019.631042	12.811994
13.781397	1021.412866	12.817011
14.304504	1012.762942	12.822029
14.088275	1014.564094	12.827047
14.011251	1007.628126	12.832064
13.773543	992.863903	12.837082
13.781490	1010.253693	12.842099
14.190396	1004.663155	12.847117
13.969861	1008.842650	12.852135
14.002048	1019.481996	12.857152
13.906959	1011.534819	12.862170
13.975058	1028.032757	12.867187
13.878238	1020.476639	12.872205
13.911862	1022.241128	12.877223
14.124795	1009.991530	12.882240
13.912791	1023.569444	12.887258
14.182003	1030.327486	12.892275
14.440902	1011.255636	12.897293
14.519199	1017.085746	12.902311
13.951075	1008.981941	12.907328
14.183324	997.123974	12.912346
14.199417	1003.127419	12.917363
14.140714	986.609023	12.922381
13.707435	984.667776	12.927399
13.846066	1005.912048	12.932416
14.123753	1012.903286	12.937434
14.065114	1015.741004	12.942451
13.872106	1014.887013	12.947469
13.894671	1012.997377	12.952487
14.188658	1011.875734	12.957504
14.374991	1014.417994	12.962522
13.948641	1013.775468	12.967539
14.044660	1019.540948	12.972557
14.112243	1015.135453	12.977575
14.164633	1030.241156	12.982592
14.503938	1042.732188	12.987610
14.441815	1053.398657	12.992627
14.561761	1040.131707	12.997645
14.385521	1028.220377	13.002663
14.135889	1022.911957	13.007680
14.381745	1026.472155	13.012698
14.413665	1045.807387	13.017715
14.640617	1036.234711	13.022733
14.596482	1036.549609	13.027751
14.602898	1031.065628	13.032768
14.773222	1010.031204	13.037786
14.123806	1015.396539	13.042803
14.449327	1018.157388	13.047821
14.430536	1023.121711	13.052839
14.186916	1024.968920	13.057856
14.583153	1036.342662	13.062874
14.378358	1060.043147	13.067891
14.480207	1049.003107	13.072909
14.755069	1038.591554	13.077927
14.556536	1045.151063	13.082944
14.839771	1047.564735	13.087962
14.501396	1049.475924	13.092979
14.976994	1044.567537	13.097997
14.879425	1042.290734	13.103015
14.720568	1045.178773	13.108032
14.877825	1011.415948	13.113050
14.407451	1019.435279	13.118067
14.449509	1036.165147	13.123085
14.369125	1039.422729	13.128103
14.308380	1033.971004	13.133120
14.405289	1041.257733	13.138138
14.733044	1049.563417	13.143155
14.797957	1045.694777	13.148173
14.590595	1048.411534	13.153191
14.481281	1053.406374	13.158208
14.578590	1040.315478	13.163226
14.461211	1045.733032	13.168243
14.503230	1052.636288	13.173261
14.693789	1067.590673	13.178279
14.964025	1075.032306	13.183296
14.967405	1070.321515	13.188314
15.155526	1075.577786	13.193331
15.097420	1065.489797	13.198349
15.144974	1070.065578	13.203367
14.938139	1068.154898	13.208384
15.129032	1047.207560	13.213402
14.701363	1040.908261	13.218419
14.980107	1059.374814	13.223437
14.841283	1055.188819	13.228455
15.029195	1056.934702	13.233472
15.128620	1067.745616	13.238490
14.837827	1073.457541	13.243507
15.518047	1065.616519	13.248525
15.255927	1060.410921	13.253543
14.856957	1047.301656	13.258560
15.204401	1053.838548	13.263578
15.335881	1051.797171	13.268595
15.089065	1044.771844	13.273613
15.022867	1042.798464	13.278631
15.099425	1049.987594	13.283648
15.168001	1058.108889	13.288666
15.006559	1066.827062	13.293683
15.209506	1065.882441	13.298701
15.460251	1058.211888	13.303719
15.233543	1075.887142	13.308736
15.278474	1062.752824	13.313754
15.186575	1073.251423	13.318771
14.963639	1078.516875	13.323789
15.032134	1072.728872	13.328807
15.048666	1077.748782	13.333824
14.858365	1064.181567	13.338842
15.178134	1077.253808	13.343859
15.389633	1069.412010	13.348877
15.420044	1071.261666	13.353895
15.190438	1070.367862	13.358912
15.397755	1063.122916	13.363930
15.016235	1065.666522	13.368947
15.213059	1073.681410	13.373965
15.677931	1079.288336	13.378983
15.852948	1085.265747	13.384000
15.788994	1084.675317	13.389018
15.332632	1081.346476	13.394035
15.478883	1059.796071	13.399053
15.551014	1055.834225	13.404071
15.349018	1078.162072	13.409088
15.221449	1058.836467	13.414106
15.433215	1067.492177	13.419123
15.184182	1080.408069	13.424141
15.496015	1095.299533	13.429159
15.665972	1100.015403	13.434176
15.781617	1097.731206	13.439194
15.635116	1102.305115	13.444211
15.492993	1097.058713	13.449229
15.951107	1096.322765	13.454247
15.817220	1102.195353	13.459264
15.411922	1101.539896	13.464282
15.859298	1104.636370	13.469299
15.864822	1110.390860	13.474317
16.032118	1099.685972	13.479335
15.559335	1091.578570	13.484352
15.756935	1095.231193	13.489370
15.876881	1092.168662	13.494387
15.816135	1097.879777	13.499405
15.785005	1085.823084	13.504423
15.490787	1091.940434	13.509440
15.321851	1094.472531	13.514458
15.449872	1100.861190	13.519475
15.622509	1092.586900	13.524493
16.229237	1095.328552	13.529511
15.999031	1105.228973	13.534528
15.978563	1098.702837	13.539546
16.231896	1104.332921	13.544563
15.809547	1104.637600	13.549581
15.777975	1089.742876	13.554599
15.946513	1102.985874	13.559616
16.279867	1095.159549	13.564634
15.933090	1102.461372	13.569651
15.729769	1103.517123	13.574669
15.946909	1105.625836	13.579687
15.961568	1101.684595	13.584704
15.943859	1098.313372	13.589722
16.279688	1096.940855	13.594739
15.924128	1096.821968	13.599757
16.287160	1096.008836	13.604775
16.072330	1096.323898	13.609792
16.218302	1095.285854	13.614810
16.292223	1098.499152	13.619827
16.013314	1117.774542	13.624845
16.198700	1095.286774	13.629863
16.179880	1102.208667	13.634880
16.167356	1101.824465	13.639898
16.012248	1099.986321	13.644915
15.958837	1104.788310	13.649933
16.020042	1096.333649	13.654951
16.153481	1116.836539	13.659968
16.010642	1122.241599	13.664986
16.172084	1123.276631	13.670003
16.072087	1134.882230	13.675021
16.903244	1123.179775	13.680039
16.365183	1131.699440	13.685056
16.609998	1130.464972	13.690074
16.743735	1130.426614	13.695091
16.586152	1128.192683	13.700109
16.638910	1108.939067	13.705127
16.393145	1109.884726	13.710144
16.274656	1099.123344	13.715162
16.232589	1103.000781	13.720179
16.360481	1121.383891	13.725197
16.756287	1125.447392	13.730215
16.606664	1122.313872	13.735232
16.452002	1126.497865	13.740250
16.423068	1129.291430	13.745267
16.614706	1133.366827	13.750285
16.743111	1125.143523	13.755303
16.416588	1139.704377	13.760320
16.603894	1126.745557	13.765338
16.605335	1131.989398	13.770355
16.441485	1139.568831	13.775373
16.644923	1126.084992	13.780391
16.720390	1127.593800	13.785408
16.482760	1138.536436	13.790426
16.558604	1132.139818	13.795443
16.206486	1142.749861	13.800461
16.628928	1135.154815	13.805479
16.607718	1137.725686	13.810496
16.454835	1136.661843	13.815514
16.494079	1135.971694	13.820531
16.529937	1142.962313	13.825549
16.572932	1159.228950	13.830567
16.757537	1167.265096	13.835584
16.809645	1165.898522	13.840602
17.151809	1156.843551	13.845619
16.760608	1168.627396	13.850637
17.251360	1154.481587	13.855655
16.953107	1161.606156	13.860672
17.033103	1169.965642	13.865690
17.247930	1165.057602	13.870707
16.954513	1140.298891	13.875725
16.992849	1129.823527	13.880743
16.418588	1140.254173	13.885760
16.622158	1154.633361	13.890778
16.837410	1156.414888	13.895795
16.701655	1153.635901	13.900813
16.925302	1157.367488	13.905831
17.256872	1166.596270	13.910848
17.200847	1167.704638	13.915866
17.119308	1156.446050	13.920883
16.889455	1161.025682	13.925901
17.125906	1156.199687	13.930919
17.009924	1155.351362	13.935936
17.111776	1158.977704	13.940954
17.314784	1168.470016	13.945971
17.174328	1157.824803	13.950989
17.383326	1156.327005	13.956007
17.243394	1160.195829	13.961024
17.181746	1152.920302	13.966042
17.228321	1153.559230	13.971059
17.472726	1164.427932	13.976077
17.296739	1147.663632	13.981095
17.643794	1161.495382	13.986112
17.651683	1161.115087	13.991130
17.497192	1160.892904	13.996147
17.276257	1164.714890	14.001165
17.091538	1168.516327	14.006183
17.468664	1154.325329	14.011200
17.335682	1156.911328	14.016218
17.703395	1159.215405	14.021235
17.267137	1162.730708	14.026253
17.481747	1161.340625	14.031271
17.257690	1157.457124	14.036288
17.302379	1159.039121	14.041306
17.429562	1155.858079	14.046323
17.109926	1169.549267	14.051341
17.255051	1173.942349	14.056359
17.437944	1186.166284	14.061376
17.161199	1199.289479	14.066394
17.608171	1191.524828	14.071411
17.502107	1190.637073	14.076429
17.517227	1188.548973	14.081447
17.623093	1196.617238	14.086464
17.630759	1185.413560	14.091482
17.759652	1177.727658	14.096499
17.526884	1193.100294	14.101517
17.730084	1188.908421	14.106535
18.105336	1180.428779	14.111552
17.927465	1192.030562	14.116570
17.961688	1186.191889	14.121587
17.764781	1192.831691	14.126605
17.682438	1196.822679	14.131623
17.782736	1187.497476	14.136640
17.632308	1184.944296	14.141658
17.853727	1179.297882	14.146675
17.943676	1192.669280	14.151693
17.722481	1190.825710	14.156711
17.570077	1181.700317	14.161728
17.567665	1180.663958	14.166746
17.692970	1199.780343	14.171763
17.799278	1219.298251	14.176781
17.902610	1209.840271	14.181799
18.073030	1217.366076	14.186816
18.124467	1224.669461	14.191834
18.416158	1209.498007	14.196851
18.222153	1222.582946	14.201869
18.016526	1218.519051	14.206887
18.635628	1205.076866	14.211904
17.856511	1183.704306	14.216922
17.767399	1192.529671	14.221939
17.990854	1199.106306	14.226957
18.200157	1207.671769	14.231975
18.439413	1223.154785	14.236992
18.412502	1220.012775	14.242010
18.478792	1196.202436	14.247027
18.282359	1196.702618	14.252045
18.067843	1190.159503	14.257063
18.349812	1182.064309	14.262080
18.077288	1194.211373	14.267098
18.642934	1198.301935	14.272115
18.571187	1183.047678	14.277133
18.449807	1184.636259	14.282151
18.598689	1172.177764	14.287168
18.335361	1175.173234	14.292186
18.477185	1167.987283	14.297203
18.387750	1178.257138	14.302221
18.342048	1173.290789	14.307239
18.048062	1177.773759	14.312256
18.270469	1178.284041	14.317274
18.773354	1191.364990	14.322291
18.441979	1192.223439	14.327309
18.173908	1193.159012	14.332327
18.522960	1200.459651	14.337344
18.223184	1207.018640	14.342362
18.645774	1200.163969	14.347379
18.556517	1207.933044	14.352397
18.459808	1202.436423	14.357415
18.804441	1196.343923	14.362432
18.489409	1205.606762	14.367450
18.428668	1202.378826	14.372467
18.759550	1204.364443	14.377485
18.495082	1202.071011	14.382503
18.693769	1209.183349	14.387520
18.585352	1216.005946	14.392538
18.654804	1205.581285	14.397555
18.409435	1210.068038	14.402573
18.851281	1202.740772	14.407591
18.910642	1199.952953	14.412608
18.346934	1222.765716	14.417626
18.486756	1209.045114	14.422643
19.107600	1215.928071	14.427661
19.210312	1228.138917	14.432679
18.881126	1217.708287	14.437696
18.511232	1213.149183	14.442714
18.734345	1222.157968	14.447731
19.029632	1233.429071	14.452749
19.130396	1240.938844	14.457767
19.278398	1232.364663	14.462784
18.480695	1235.003447	14.467802
18.654541	1245.312109	14.472819
18.874365	1231.559962	14.477837
19.244749	1235.881196	14.482855
19.104626	1229.193311	14.487872
19.067552	1237.304311	14.492890
19.128931	1224.123542	14.497907
19.154580	1240.524016	14.502925
19.127586	1238.145476	14.507943
19.237250	1237.273043	14.512960
19.297631	1235.808851	14.517978
19.158793	1234.828297	14.522995
19.397315	1224.955903	14.528013
19.295836	1230.195333	14.533031
19.419671	1230.812443	14.538048
19.329391	1233.114474	14.543066
19.076060	1235.949865	14.548083
19.391601	1235.668899	14.553101
19.233582	1242.064539	14.558119
19.183865	1232.019928	14.563136
19.156116	1246.092405	14.568154
19.281609	1240.370301	14.573171
19.213587	1242.433260	14.578189
19.075993	1245.626631	14.583207
19.454829	1234.272421	14.588224
19.636910	1240.396536	14.593242
19.590979	1240.239665	14.598259
19.378732	1234.085267	14.603277
19.177709	1235.160328	14.608295
19.380845	1233.619208	14.613312
19.195042	1239.697246	14.618330
19.468323	1252.102131	14.623347
19.608140	1257.206434	14.628365
19.728863	1264.133091	14.633383
19.953191	1254.402373	14.638400
19.690783	1252.811827	14.643418
19.795933	1239.325828	14.648435
19.444223	1232.086979	14.653453
19.504510	1241.290177	14.658471
19.607494	1250.538678	14.663488
19.799410	1263.446311	14.668506
19.758916	1259.517884	14.673523
20.189982	1253.539404	14.678541
19.958265	1260.618973	14.683559
20.066710	1242.458567	14.688576
19.854930	1231.129927	14.693594
19.879998	1217.477879	14.698611
19.813208	1227.240958	14.703629
19.837298	1228.463826	14.708647
19.968632	1222.821262	14.713664
19.779224	1232.128306	14.718682
19.980455	1250.057594	14.723699
20.391176	1239.507625	14.728717
20.041604	1232.853565	14.733735
20.287851	1226.587186	14.738752
19.750353	1220.842981	14.743770
19.690739	1221.647862	14.748787
20.315730	1226.398595	14.753805
20.307651	1241.602083	14.758823
20.190133	1236.699542	14.763840
20.171582	1227.906667	14.768858
20.035659	1218.999555	14.773875
20.239510	1224.029692	14.778893
20.057090	1239.969748	14.783911
20.350900	1244.233965	14.788928
20.284752	1232.933020	14.793946
20.255139	1242.494524	14.798963
20.842308	1222.914890	14.803981
20.613991	1227.712166	14.808999
20.586167	1212.876536	14.814016
20.305554	1222.923726	14.819034
20.294726	1217.098391	14.824051
20.082607	1211.385248	14.829069
20.218615	1223.218011	14.834087
20.465814	1213.913193	14.839104
20.458273	1206.297847	14.844122
20.327796	1219.753325	14.849139
20.535259	1212.296508	14.854157
20.270842	1205.457155	14.859175
20.156725	1214.855273	14.864192
20.459585	1214.656115	14.869210
20.386862	1241.062956	14.874227
20.241542	1249.263690	14.879245
20.086464	1250.883039	14.884263
20.550512	1245.958588	14.889280
20.504103	1252.585156	14.894298
20.298898	1254.893586	14.899315
20.476745	1255.633641	14.904333
20.177936	1252.431259	14.909351
20.626901	1253.138712	14.914368
20.662251	1255.160381	14.919386
20.799722	1256.165727	14.924403
21.227656	1266.417062	14.929421
20.633707	1254.356608	14.934439
20.663508	1242.781769	14.939456
20.770102	1245.604525	14.944474
20.473714	1266.795674	14.949491
21.255320	1254.940705	14.954509
21.342416	1261.475935	14.959527
20.977003	1255.220875	14.964544
21.303151	1238.236115	14.969562
20.929676	1240.689261	14.974579
20.827698	1232.012910	14.979597
20.682647	1243.950788	14.984615
20.701273	1240.058652	14.989632
21.124343	1250.665053	14.994650
21.085374	1255.267490	14.999667
20.965500	1254.571943	15.004685
21.010719	1270.660012	15.009703
21.221872	1275.471868	15.014720
21.329458	1262.761701	15.019738
21.305750	1268.159523	15.024755
21.168134	1254.800033	15.029773
21.073026	1249.428111	15.034791
21.357344	1258.189833	15.039808
21.250099	1254.942213	15.044826
21.153460	1258.904876	15.049843
21.122990	1259.560674	15.054861
21.187539	1268.047157	15.059879
21.534010	1275.122900	15.064896
21.430280	1257.938335	15.069914
21.318615	1262.344947	15.074931
21.414917	1263.859380	15.079949
21.620521	1270.382508	15.084967
21.087751	1276.285062	15.089984
21.525561	1271.575535	15.095002
21.361784	1269.470736	15.100019
21.456454	1266.443445	15.105037
21.323530	1262.557847	15.110055
21.322562	1266.987695	15.115072
21.809852	1263.208624	15.120090
21.538591	1268.650309	15.125107
21.404798	1259.384610	15.130125
21.617045	1271.148914	15.135143
21.289087	1270.013027	15.140160
21.550443	1273.702983	15.145178
21.353595	1268.449426	15.150195
21.200380	1261.823130	15.155213
21.401991	1270.887655	15.160231
21.693665	1297.207212	15.165248
21.550995	1307.769569	15.170266
21.767466	1309.307841	15.175283
21.892637	1312.687885	15.180301
22.128810	1303.510800	15.185319
21.670061	1287.509301	15.190336
21.791641	1290.588012	15.195354
21.525084	1298.469096	15.200371
21.905423	1292.181712	15.205389
22.112367	1289.976872	15.210407
21.891633	1287.108770	15.215424
22.091425	1288.724982	15.220442
22.272708	1294.467618	15.225459
22.448622	1287.297824	15.230477
21.900450	1274.756045	15.235495
22.049107	1260.091173	15.240512
21.917044	1246.289504	15.245530
21.790901	1264.658477	15.250547
21.916753	1281.357740	15.255565
22.257215	1297.539741	15.260583
21.860170	1295.199514	15.265600
22.314108	1281.682999	15.270618
21.962402	1294.201240	15.275635
22.397423	1285.427653	15.280653
22.082876	1285.655277	15.285671
21.911394	1298.732425	15.290688
22.102298	1286.707965	15.295706
21.835226	1290.586417	15.300723
22.002996	1292.246104	15.305741
21.907252	1280.501463	15.310759
22.219757	1292.163993	15.315776
22.448244	1315.361053	15.320794
22.620945	1321.670581	15.325811
22.659259	1316.969195	15.330829
22.687255	1309.722669	15.335847
22.129887	1304.096463	15.340864
22.598503	1291.940095	15.345882
22.463288	1313.529606	15.350899
22.380540	1317.493925	15.355917
22.593254	1311.332447	15.360935
22.488888	1313.606310	15.365952
23.134792	1316.983949	15.370970
22.581897	1320.524269	15.375987
22.879797	1315.728419	15.381005
22.704546	1307.726826	15.386023
22.665031	1309.009614	15.391040
22.849217	1291.858126	15.396058
22.456950	1301.412286	15.401075
22.782544	1317.798898	15.406093
22.818241	1308.771654	15.411111
22.821627	1318.721785	15.416128
22.909468	1318.389484	15.421146
22.711523	1314.795086	15.426163
23.197419	1310.900897	15.431181
23.141887	1313.810685	15.436199
22.925714	1303.072388	15.441216
23.087630	1284.902309	15.446234
22.572754	1284.095490	15.451251
22.866099	1307.886253	15.456269
23.159595	1314.548395	15.461287
22.850267	1312.605220	15.466304
22.702761	1304.662616	15.471322
22.693469	1322.978692	15.476339
22.918289	1304.535440	15.481357
22.938117	1314.448210	15.486375
22.666822	1312.285004	15.491392
22.964868	1307.587148	15.496410
22.566080	1322.555133	15.501427
22.845739	1332.002207	15.506445
23.439682	1344.587408	15.511463
23.429386	1356.133672	15.516480
23.708245	1347.660618	15.521498
23.513321	1343.953526	15.526515
23.345360	1323.629595	15.531533
23.424788	1310.211357	15.536551
23.262424	1311.384742	15.541568
23.434083	1314.808867	15.546586
23.413946	1314.157849	15.551603
23.099368	1316.980939	15.556621
23.402468	1324.717708	15.561639
23.271362	1347.416062	15.566656
23.559014	1338.375505	15.571674
23.374249	1338.410055	15.576691
23.186891	1350.345953	15.581709
23.305208	1342.107274	15.586727
22.966040	1343.599206	15.591744
23.756455	1345.840148	15.596762
23.895740	1347.290408	15.601779
23.839481	1342.689079	15.606797
23.818606	1333.589489	15.611815
23.491985	1339.669187	15.616832
23.771965	1335.557682	15.621850
23.786975	1338.737859	15.626867
23.700180	1343.091966	15.631885
23.618818	1340.170315	15.636903
23.307292	1339.006120	15.641920
23.579583	1342.078633	15.646938
23.762382	1365.937747	15.651955
23.959811	1367.311087	15.656973
24.297811	1374.153864	15.661991
23.827714	1361.624501	15.667008
23.907393	1362.495923	15.672026
24.071902	1361.766365	15.677043
23.974414	1362.229534	15.682061
24.144786	1362.502397	15.687079
24.163950	1374.697643	15.692096
24.326789	1368.843355	15.697114
23.794185	1346.736431	15.702131
24.086897	1362.879548	15.707149
24.365859	1365.413841	15.712167
24.033939	1368.039246	15.717184
24.423539	1368.776198	15.722202
24.298906	1359.660673	15.727219
23.862899	1354.797146	15.732237
24.022351	1355.988207	15.737255
23.438900	1377.756001	15.742272
24.075901	1359.229412	15.747290
24.124264	1358.118519	15.752307
24.151703	1372.764383	15.757325
24.294803	1353.446130	15.762343
24.085336	1370.177678	15.767360
24.306426	1388.322709	15.772378
24.457345	1389.048128	15.777395
24.598094	1395.616078	15.782413
24.876468	1389.157344	15.787431
24.824177	1377.905963	15.792448
24.463967	1364.076153	15.797466
24.641924	1369.758943	15.802483
24.525448	1371.246157	15.807501
24.533650	1349.981210	15.812519
24.405481	1367.590719	15.817536
24.617237	1384.569947	15.822554
24.767621	1387.064281	15.827571
24.847237	1396.004967	15.832589
25.045758	1388.709755	15.837607
24.537421	1400.629849	15.842624
24.790175	1395.037815	15.847642
24.870462	1379.362629	15.852659
24.775959	1396.669605	15.857677
24.996362	1397.041665	15.862695
24.861077	1394.497166	15.867712
24.973233	1390.490731	15.872730
25.171416	1391.363041	15.877747
24.731447	1389.946290	15.882765
24.951884	1379.422752	15.887783
24.671722	1399.619033	15.892800
25.127772	1397.264564	15.897818
25.312869	1382.563243	15.902835
25.387669	1387.001271	15.907853
25.360057	1374.396215	15.912871
24.615601	1365.199483	15.917888
24.803338	1372.329846	15.922906
25.142287	1389.856478	15.927923
25.081997	1391.043902	15.932941
25.079348	1376.333659	15.937959
25.008607	1383.151481	15.942976
24.999465	1387.527999	15.947994
25.143723	1379.211993	15.953011
25.074306	1393.271612	15.958029
25.334091	1385.318934	15.963047
25.409949	1382.414988	15.968064
25.181071	1385.500657	15.973082
25.193921	1392.911270	15.978099
25.168810	1409.364007	15.983117
25.671003	1405.027207	15.988135
25.426846	1404.153993	15.993152
25.271281	1408.736577	15.998170
25.557485	1405.085373	16.003187
25.422191	1416.267752	16.008205
25.577899	1414.842309	16.013223
25.524781	1418.237668	16.018240
25.685854	1424.947722	16.023258
25.875529	1406.500512	16.028275
25.373512	1415.538706	16.033293
25.643821	1418.749140	16.038311
25.462807	1411.183027	16.043328
25.359576	1407.909321	16.048346
25.729052	1412.989894	16.053363
25.779807	1413.358498	16.058381
25.787638	1405.412216	16.063399
25.507962	1416.577713	16.068416
25.866627	1422.413113	16.073434
26.026852	1435.510746	16.078451
25.663036	1452.335006	16.083469
26.160554	1436.266647	16.088487
26.036358	1442.751254	16.093504
26.119917	1442.849320	16.098522
26.253957	1427.692486	16.103539
26.112697	1448.551799	16.108557
26.193011	1436.981456	16.113575
26.246084	1425.546314	16.118592
25.919243	1440.244688	16.123610
26.206000	1432.566818	16.128627
26.108317	1439.064953	16.133645
26.629978	1440.953532	16.138663
26.694085	1437.037888	16.143680
26.278033	1424.573546	16.148698
26.162151	1406.980254	16.153715
25.978348	1414.800091	16.158733
26.121983	1425.289431	16.163751
26.536785	1434.729194	16.168768
26.386626	1432.395186	16.173786
26.491373	1428.136461	16.178803
25.919251	1438.466772	16.183821
26.552126	1435.773475	16.188839
26.729838	1435.453088	16.193856
26.222310	1443.588013	16.198874
26.532997	1432.183708	16.203891
26.257201	1444.485423	16.208909
26.483127	1434.896235	16.213927
26.718805	1432.857073	16.218944
26.534660	1441.194423	16.223962
26.731523	1435.138650	16.228979
26.484853	1442.855128	16.233997
26.948934	1443.009190	16.239015
26.958410	1438.311548	16.244032
26.670182	1442.978851	16.249050
26.923676	1442.966760	16.254067
26.574103	1431.828827	16.259085
26.641954	1425.748912	16.264103
26.556617	1437.777647	16.269120
26.653369	1459.664610	16.274138
27.184605	1463.312572	16.279155
27.057452	1465.347542	16.284173
27.659164	1468.096981	16.289191
27.244298	1449.367396	16.294208
26.979968	1427.390798	16.299226
27.005263	1434.763357	16.304243
26.921652	1435.245885	16.309261
27.058654	1424.214332	16.314279
27.091796	1427.987899	16.319296
27.216305	1445.770669	16.324314
27.403074	1457.879828	16.329331
27.105280	1446.742775	16.334349
27.313676	1446.174833	16.339367
27.423230	1450.899219	16.344384
27.220623	1460.418984	16.349402
27.331088	1455.151187	16.354419
27.257871	1461.572661	16.359437
27.328875	1457.092961	16.364455
27.248236	1447.014153	16.369472
27.245711	1457.948079	16.374490
27.701762	1450.180028	16.379507
27.083233	1456.192674	16.384525
27.528314	1462.174414	16.389543
27.601542	1449.224531	16.394560
27.509611	1458.167032	16.399578
27.933183	1446.351600	16.404595
27.681033	1453.119326	16.409613
27.575194	1451.562324	16.414631
27.975367	1455.425616	16.419648
27.537359	1458.363996	16.424666
27.695668	1452.043762	16.429683
27.723580	1455.131884	16.434701
27.687718	1458.852108	16.439719
27.759940	1456.673051	16.444736
27.420826	1457.432217	16.449754
27.672234	1452.928021	16.454771
27.541450	1454.723074	16.459789
27.814854	1472.386008	16.464807
28.071922	1480.674478	16.469824
27.682835	1492.089966	16.474842
27.927095	1480.876104	16.479859
27.763338	1486.386504	16.484877
27.631137	1485.862841	16.489895
27.824903	1484.820022	16.494912
27.681729	1469.987264	16.499930
28.216334	1480.018388	16.504947
28.073285	1482.535643	16.509965
28.344391	1487.096945	16.514983
28.194108	1490.688863	16.520000
28.104179	1504.252636	16.525018
28.258007	1507.910820	16.530035
28.511604	1507.108864	16.535053
28.561965	1517.643795	16.540071
28.098097	1493.105173	16.545088
28.236723	1498.430981	16.550106
28.651396	1504.565380	16.555123
28.623114	1506.367316	16.560141
28.547582	1505.133994	16.565159
28.805761	1489.097457	16.570176
28.282597	1490.618037	16.575194
28.496994	1488.295812	16.580211
28.575589	1509.629431	16.585229
28.505295	1501.416129	16.590247
29.051540	1489.986238	16.595264
28.708078	1498.285980	16.600282
28.633918	1492.421211	16.605299
28.563742	1506.034469	16.610317
28.580764	1518.925754	16.615335
28.655204	1505.733335	16.620352
28.543938	1501.554177	16.625370
28.925144	1502.906214	16.630387
29.107137	1500.567496	16.635405
28.918146	1506.677460	16.640423
29.210626	1515.531669	16.645440
28.901982	1509.984737	16.650458
29.094949	1500.906197	16.655475
29.077452	1509.010168	16.660493
29.023409	1499.136940	16.665511
29.330427	1493.299520	16.670528
28.994983	1507.947419	16.675546
29.150817	1506.016508	16.680563
28.967546	1499.630672	16.685581
28.922109	1503.507191	16.690599
29.262645	1504.928932	16.695616
29.064439	1501.398500	16.700634
29.280156	1496.759461	16.705651
29.169710	1502.499408	16.710669
29.030294	1506.210186	16.715687
29.241506	1480.011231	16.720704
28.988471	1504.383465	16.725722
29.364385	1520.769459	16.730739
29.704465	1532.132775	16.735757
29.503974	1535.891442	16.740775
29.269554	1534.290927	16.745792
29.274163	1534.415227	16.750810
29.541171	1530.199334	16.755827
29.730087	1527.259749	16.760845
29.490731	1533.454808	16.765863
29.922971	1531.794510	16.770880
29.357549	1540.886359	16.775898
29.533400	1525.530618	16.780915
29.929342	1529.753041	16.785933
29.484690	1527.441705	16.790951
29.757724	1521.430192	16.795968
29.720127	1532.243410	16.800986
29.877677	1536.643597	16.806003
29.764391	1528.507454	16.811021
29.657238	1531.172699	16.816039
29.964003	1529.865767	16.821056
29.789800	1544.184144	16.826074
29.762761	1532.622024	16.831091
30.170592	1542.113589	16.836109
30.053833	1551.677089	16.841127
30.332118	1560.673611	16.846144
29.800240	1547.642959	16.851162
30.164712	1555.855658	16.856179
30.197529	1550.873456	16.861197
29.966629	1567.218853	16.866215
30.375835	1553.898443	16.871232
30.197578	1562.238625	16.876250
30.139110	1561.620306	16.881267
30.169653	1563.592029	16.886285
30.142203	1566.366139	16.891303
30.512661	1564.553866	16.896320
30.296761	1556.575787	16.901338
30.394769	1558.385398	16.906355
30.142039	1554.226849	16.911373
29.890762	1557.114904	16.916391
30.323601	1558.376141	16.921408
30.395193	1564.488925	16.926426
30.166133	1578.684135	16.931443
30.652179	1584.801064	16.936461
31.070637	1587.443820	16.941479
31.060924	1573.548616	16.946496
30.959188	1570.237233	16.951514
30.817133	1553.066347	16.956531
30.952220	1550.679672	16.961549
30.828608	1553.086457	16.966567
31.176314	1550.985270	16.971584
31.081571	1553.980114	16.976602
30.884765	1544.498901	16.981619
31.141710	1553.619991	16.986637
31.077869	1548.384509	16.991655
30.871693	1551.186381	16.996672
30.668909	1549.806391	17.001690
30.633322	1545.774929	17.006707
30.805647	1548.200319	17.011725
30.978841	1570.997118	17.016743
31.324534	1576.093092	17.021760
31.010050	1577.156025	17.026778
31.154597	1585.313561	17.031795
31.400633	1578.433774	17.036813
30.992078	1582.976732	17.041831
31.440279	1583.609142	17.046848
31.223329	1582.323604	17.051866
31.115389	1579.481682	17.056883
31.237237	1581.209021	17.061901
31.307399	1584.706074	17.066919
31.352471	1579.334686	17.071936
31.076064	1575.647301	17.076954
30.815315	1587.146361	17.081971
31.277737	1597.166856	17.086989
31.655624	1599.410469	17.092007
31.597371	1609.307596	17.097024
31.612282	1607.219277	17.102042
31.978994	1615.232847	17.107059
31.664738	1605.742466	17.112077
31.636099	1610.956406	17.117095
31.879229	1609.755836	17.122112
31.710766	1609.633973	17.127130
31.527240	1616.706922	17.132147
31.909171	1610.910024	17.137165
31.673079	1607.052999	17.142183
31.707553	1606.897206	17.147200
31.915568	1616.483640	17.152218
31.555795	1613.767962	17.157235
32.014690	1609.681733	17.162253
31.825369	1609.587919	17.167271
31.870762	1614.256629	17.172288
31.972704	1619.993604	17.177306
31.915922	1628.937284	17.182323
32.344800	1635.570305	17.187341
32.093766	1640.956225	17.192359
32.332629	1646.859337	17.197376
32.673043	1645.605489	17.202394
32.284902	1643.133045	17.207411
32.289354	1632.333652	17.212429
32.488155	1627.817038	17.217447
32.345202	1620.296296	17.222464
32.354762	1614.834518	17.227482
32.365082	1634.052717	17.232499
32.600400	1638.630214	17.237517
32.359536	1643.597976	17.242535
32.257419	1644.687817	17.247552
32.298929	1647.585371	17.252570
32.264817	1633.024944	17.257587
32.900433	1638.971332	17.262605
32.524606	1637.932880	17.267623
32.727041	1626.634498	17.272640
32.707359	1632.946029	17.277658
32.550548	1637.174209	17.282675
32.923213	1627.241011	17.287693
32.856221	1636.346401	17.292711
32.604053	1631.330963	17.297728
32.716143	1633.493523	17.302746
32.472209	1633.543165	17.307763
32.655354	1640.946422	17.312781
32.698449	1642.399026	17.317799
32.770271	1648.803301	17.322816
33.049556	1648.638543	17.327834
32.873436	1656.926855	17.332851
32.957517	1654.643068	17.337869
33.212525	1648.843512	17.342887
32.852150	1650.863315	17.347904
33.350155	1646.846783	17.352922
32.909753	1647.330413	17.357939
33.552209	1642.278140	17.362957
33.169134	1649.986164	17.367975
33.227281	1651.596889	17.372992
33.563209	1633.223060	17.378010
33.427613	1640.069822	17.383027
33.203478	1642.331443	17.388045
33.290915	1645.487906	17.393063
32.840323	1648.335303	17.398080
33.561074	1665.622014	17.403098
33.831783	1667.607992	17.408115
33.767361	1662.613087	17.413133
34.043087	1681.875861	17.418151
33.796446	1665.613157	17.423168
33.888889	1635.989339	17.428186
33.933402	1648.690585	17.433203
33.670748	1640.742233	17.438221
33.703144	1634.806068	17.443239
33.938935	1646.004444	17.448256
33.623661	1656.868361	17.453274
34.306254	1666.434266	17.458291
34.247576	1646.198724	17.463309
34.179167	1640.705339	17.468327
33.800790	1640.496921	17.473344
34.116504	1622.772420	17.478362
33.860364	1640.356151	17.483379
34.011572	1653.415505	17.488397
34.026852	1666.075735	17.493415
34.023228	1669.267130	17.498432
34.114664	1662.379788	17.503450
33.859068	1655.218543	17.508467
34.259286	1661.907486	17.513485
34.574619	1674.741927	17.518503
34.393141	1665.471660	17.523520
34.498352	1672.157003	17.528538
34.256435	1670.422297	17.533555
34.392394	1657.629763	17.538573
34.260845	1666.636996	17.543591
34.450293	1663.058013	17.548608
34.270922	1653.306761	17.553626
33.896733	1658.712252	17.558643
34.377515	1677.604565	17.563661
34.418070	1688.648253	17.568679
34.404743	1706.222046	17.573696
34.755730	1702.827945	17.578714
34.418700	1696.102524	17.583731
34.492264	1711.669313	17.588749
34.858039	1707.238651	17.593767
34.386772	1702.973477	17.598784
34.908043	1694.807569	17.603802
34.594840	1705.720187	17.608819
34.659772	1698.326449	17.613837
35.149234	1705.667111	17.618855
34.686128	1723.639619	17.623872
34.834688	1725.881390	17.628890
34.797564	1724.973156	17.633907
35.239311	1737.952290	17.638925
34.899663	1735.031913	17.643943
34.979314	1742.971153	17.648960
35.299657	1738.488155	17.653978
35.396463	1733.033961	17.658995
34.970561	1726.689504	17.664013
35.016817	1738.184392	17.669031
34.951735	1735.464083	17.674048
35.223259	1724.897029	17.679066
35.363969	1734.727307	17.684083
35.408501	1747.559322	17.689101
35.468578	1753.900236	17.694119
35.579831	1745.693215	17.699136
36.040589	1747.731055	17.704154
35.754045	1747.908588	17.709171
35.732073	1743.815777	17.714189
36.126744	1718.730638	17.719207
35.628337	1724.485574	17.724224
36.096862	1719.698996	17.729242
35.825994	1709.520563	17.734259
35.763074	1716.920628	17.739277
35.852588	1713.424282	17.744295
35.490520	1711.622233	17.749312
35.959856	1727.134460	17.754330
36.129248	1741.506855	17.759347
36.309196	1734.944771	17.764365
36.426723	1718.346275	17.769383
35.899619	1728.033594	17.774400
36.034193	1710.483594	17.779418
35.831749	1711.131221	17.784435
36.021957	1734.629888	17.789453
36.196461	1736.155063	17.794471
36.276574	1744.510710	17.799488
36.514229	1740.453134	17.804506
36.420694	1733.958682	17.809523
36.453851	1743.932904	17.814541
36.405947	1745.005724	17.819559
36.370721	1746.324646	17.824576
36.197596	1734.919569	17.829594
36.482240	1745.938510	17.834611
36.253077	1737.632846	17.839629
36.943716	1739.968086	17.844647
36.203751	1750.042125	17.849664
36.373881	1739.059786	17.854682
36.235320	1739.391582	17.859699
36.568198	1744.464143	17.864717
37.016065	1734.462747	17.869735
36.747143	1735.845284	17.874752
36.814675	1734.719387	17.879770
36.939804	1741.688637	17.884787
36.566202	1734.235675	17.889805
37.112849	1736.587033	17.894823
36.587808	1741.072131	17.899840
37.254518	1737.563652	17.904858
36.955436	1758.809655	17.909875
37.002060	1769.110563	17.914893
37.389917	1761.050909	17.919911
36.742581	1757.393482	17.924928
37.050615	1766.143901	17.929946
37.153740	1759.886590	17.934963
37.081500	1766.415890	17.939981
37.013073	1762.703538	17.944999
37.204896	1760.633988	17.950016
37.355045	1758.397922	17.955034
37.335169	1760.060524	17.960051
37.389826	1773.499275	17.965069
37.531389	1753.494247	17.970087
37.407427	1759.931907	17.975104
37.253622	1759.439753	17.980122
36.978114	1754.375580	17.985139
37.044330	1770.392601	17.990157
37.527719	1778.173223	17.995175
37.563964	1795.747980	18.000192
37.699509	1790.762108	18.005210
37.931703	1784.456886	18.010227
37.609507	1783.313116	18.015245
37.876705	1787.917472	18.020263
37.920659	1785.200983	18.025280
38.141155	1782.267548	18.030298
38.248565	1780.043856	18.035315
38.057774	1787.270820	18.040333
38.517015	1772.798593	18.045351
38.220505	1779.459042	18.050368
38.246252	1782.322419	18.055386
38.409171	1769.031109	18.060403
38.352711	1773.659029	18.065421
38.594767	1761.660190	18.070439
38.085606	1748.775593	18.075456
38.114641	1755.745771	18.080474
38.300575	1761.006182	18.085491
38.188999	1769.407692	18.090509
38.426197	1778.962834	18.095527
38.183488	1784.160050	18.100544
37.930916	1779.266859	18.105562
38.364786	1772.616346	18.110579
38.235020	1784.817831	18.115597
38.109060	1768.606325	18.120615
38.417214	1782.600755	18.125632
38.600788	1796.539810	18.130650
38.617827	1810.842381	18.135667
38.445359	1809.123540	18.140685
38.594757	1808.984772	18.145703
38.774057	1808.510198	18.150720
38.653430	1811.646558	18.155738
38.900763	1807.760572	18.160755
38.559924	1815.086549	18.165773
38.809354	1804.833486	18.170791
38.832739	1807.926364	18.175808
38.797244	1830.701546	18.180826
39.196670	1826.807743	18.185843
39.009318	1834.403800	18.190861
39.179442	1832.364398	18.195879
39.505397	1833.583881	18.200896
39.065076	1831.050549	18.205914
38.875143	1835.698576	18.210931
38.927828	1835.541346	18.215949
39.389050	1822.058979	18.220967
39.297632	1827.025918	18.225984
39.286437	1837.223449	18.231002
39.827566	1821.796420	18.236019
39.329702	1836.280352	18.241037
39.721454	1830.779942	18.246055
39.763613	1824.085490	18.251072
39.905066	1828.330370	18.256090
39.949561	1828.302824	18.261107
39.597001	1829.145124	18.266125
39.746959	1830.072471	18.271143
39.960354	1837.582032	18.276160
39.537409	1832.799842	18.281178
39.799120	1830.095385	18.286195
39.432306	1839.616736	18.291213
39.618281	1822.811565	18.296231
39.547101	1834.270820	18.301248
39.693542	1849.776105	18.306266
39.636632	1852.373267	18.311283
39.759661	1868.586489	18.316301
40.333114	1865.902548	18.321319
39.732616	1861.108554	18.326336
39.695415	1863.824100	18.331354
40.345619	1863.019177	18.336371
39.880548	1865.609392	18.341389
40.149579	1872.226417	18.346407
40.538151	1891.162968	18.351424
40.680888	1891.548860	18.356442
41.018264	1885.514960	18.361459
40.506053	1878.355471	18.366477
40.287795	1866.914649	18.371495
40.719978	1877.980358	18.376512
40.681242	1880.310971	18.381530
40.877003	1885.676875	18.386547
40.436463	1894.792185	18.391565
40.694133	1887.527707	18.396583
41.132889	1887.519840	18.401600
40.623485	1882.963118	18.406618
41.116601	1883.038973	18.411635
41.172165	1885.856108	18.416653
41.105509	1874.992714	18.421671
41.022361	1861.527840	18.426688
40.858576	1858.610066	18.431706
41.209652	1876.629482	18.436723
41.122726	1892.331624	18.441741
41.227892	1884.899458	18.446759
41.329510	1881.727413	18.451776
41.097890	1881.439036	18.456794
41.167963	1872.639611	18.461811
40.914991	1880.623064	18.466829
41.235653	1874.397663	18.471847
41.412958	1879.661903	18.476864
41.008680	1888.850932	18.481882
41.037207	1879.687547	18.486899
40.960961	1876.337046	18.491917
41.491283	1899.140859	18.496935
41.270420	1916.362619	18.501952
41.332920	1917.600650	18.506970
41.450766	1912.167323	18.511987
41.520861	1919.599828	18.517005
41.315242	1916.914127	18.522023
41.744009	1917.690299	18.527040
41.231305	1914.782936	18.532058
42.053551	1923.465593	18.537075
41.752189	1946.238430	18.542093
41.671338	1945.240176	18.547111
42.297778	1931.493825	18.552128
42.352243	1940.441543	18.557146
42.375253	1929.591243	18.562163
42.283249	1933.371050	18.567181
41.971424	1933.882055	18.572199
42.369733	1933.606495	18.577216
42.235053	1924.383449	18.582234
42.376495	1924.501084	18.587251
42.450716	1932.061836	18.592269
42.402025	1923.479820	18.597287
42.486827	1916.284441	18.602304
42.730544	1932.876952	18.607322
42.415715	1913.061298	18.612339
42.719727	1906.392232	18.617357
42.347669	1908.221304	18.622375
42.349519	1903.597213	18.627392
42.684508	1915.059281	18.632410
42.588893	1926.701165	18.637427
42.724287	1936.941459	18.642445
42.426631	1930.815459	18.647463
42.556859	1920.655632	18.652480
42.840302	1939.411214	18.657498
42.735927	1930.837018	18.662515
42.804879	1932.506610	18.667533
42.607880	1930.154482	18.672551
42.611150	1937.730702	18.677568
42.663857	1948.544248	18.682586
42.930354	1966.344899	18.687603
42.769067	1976.862173	18.692621
42.832213	1973.295134	18.697639
43.168250	1961.480784	18.702656
42.953453	1973.655136	18.707674
43.241929	1969.636735	18.712691
43.237609	1984.567138	18.717709
43.433044	1992.186226	18.722727
43.754337	1991.710817	18.727744
43.525957	1999.585161	18.732762
43.716467	1985.004407	18.737779
43.833793	1994.713926	18.742797
43.560664	2002.613381	18.747815
43.900581	1983.169896	18.752832
43.628380	2002.261049	18.757850
44.074549	1995.818228	18.762867
43.722084	1992.515907	18.767885
43.825295	1993.470278	18.772903
44.192084	1995.985243	18.777920
43.926379	1990.403878	18.782938
44.220767	1986.519520	18.787955
44.286959	1976.584191	18.792973
43.800525	1963.843081	18.797991
44.052177	1980.375480	18.803008
44.062968	1982.138144	18.808026
44.232506	1984.024952	18.813043
44.201401	1995.522384	18.818061
44.066395	1992.532514	18.823079
44.109623	1991.714320	18.828096
44.178142	1989.735187	18.833114
44.324511	1987.334771	18.838131
44.168044	1998.521464	18.843149
43.938461	1995.301186	18.848167
44.187938	1997.906987	18.853184
44.258007	2021.487748	18.858202
44.524126	2025.989610	18.863219
44.618876	2021.424927	18.868237
44.345020	2017.505936	18.873255
44.403095	2023.856740	18.878272
44.402875	2024.441831	18.883290
44.513877	2029.857812	18.888307
44.794345	2045.472628	18.893325
44.694131	2048.771785	18.898343
44.857526	2041.466128	18.903360
44.941751	2053.008907	18.908378
45.418433	2041.163775	18.913395
45.224605	2040.062151	18.918413
45.032498	2046.719240	18.923431
45.090927	2045.516093	18.928448
45.262188	2040.966119	18.933466
45.290231	2051.356104	18.938483
45.377248	2045.909913	18.943501
45.111608	2046.604804	18.948519
45.110748	2047.043561	18.953536
45.124557	2050.292974	18.958554
45.254678	2070.599675	18.963571
45.511896	2076.309782	18.968589
45.652177	2078.032557	18.973607
45.562431	2071.052546	18.978624
45.738277	2077.416583	18.983642
45.644550	2080.295626	18.988659
45.832325	2067.471161	18.993677
45.611179	2079.053008	18.998695
45.707863	2065.977090	19.003712
45.554784	2073.942167	19.008730
45.342726	2069.681490	19.013747
45.715826	2084.329170	19.018765
45.757935	2095.892720	19.023783
46.084458	2098.663740	19.028800
45.915861	2096.809202	19.033818
46.086816	2094.955632	19.038835
46.368138	2103.220159	19.043853
46.199968	2097.049862	19.048871
46.414863	2086.831255	19.053888
46.367507	2100.783356	19.058906
46.294059	2107.064994	19.063923
46.567066	2100.018331	19.068941
46.643075	2095.782476	19.073959
46.769632	2093.900618	19.078976
46.373820	2092.635342	19.083994
46.556050	2094.590924	19.089011
46.399205	2103.796075	19.094029
46.354457	2111.724570	19.099047
46.676619	2126.365749	19.104064
46.771143	2131.076885	19.109082
46.645503	2126.809588	19.114099
46.918547	2127.523523	19.119117
46.867022	2131.684838	19.124135
46.750811	2122.221245	19.129152
46.971721	2129.682073	19.134170
46.943591	2137.948352	19.139187
46.774205	2128.994475	19.144205
47.183835	2144.754761	19.149223
47.461070	2150.123435	19.154240
47.643658	2151.857334	19.159258
47.430558	2152.522093	19.164275
47.753938	2148.097525	19.169293
47.532857	2156.389204	19.174311
47.754827	2143.267126	19.179328
47.682757	2137.251978	19.184346
47.441879	2138.381122	19.189363
47.546111	2133.804406	19.194381
47.457434	2154.069232	19.199399
47.679079	2157.705933	19.204416
47.961759	2144.938548	19.209434
47.771540	2153.515253	19.214451
48.009763	2144.792206	19.219469
47.693163	2148.535960	19.224487
48.056978	2143.929139	19.229504
47.908981	2146.423107	19.234522
47.898730	2137.965512	19.239539
48.221268	2139.124962	19.244557
47.925362	2151.064260	19.249575
48.048588	2135.251893	19.254592
47.740402	2138.687199	19.259610
47.968845	2156.425468	19.264627
48.282330	2163.646037	19.269645
48.250723	2179.732006	19.274663
48.371458	2176.466396	19.279680
48.356578	2167.686747	19.284698
48.704813	2179.669409	19.289715
48.760181	2175.450918	19.294733
48.342276	2168.581189	19.299751
48.150482	2175.077667	19.304768
48.867992	2164.999746	19.309786
48.426449	2171.776643	19.314803
48.538807	2167.807175	19.319821
48.590840	2180.761921	19.324839
48.729738	2182.989020	19.329856
49.174350	2197.743877	19.334874
49.143179	2195.307223	19.339891
49.375200	2200.450338	19.344909
48.638690	2205.526758	19.349927
49.008357	2199.233096	19.354944
49.520114	2193.269858	19.359962
49.154593	2204.149153	19.364979
49.291168	2187.889098	19.369997
49.465066	2196.892615	19.375015
49.326195	2201.664584	19.380032
49.471132	2191.871600	19.385050
49.701494	2198.253645	19.390067
49.689208	2200.216585	19.395085
49.695078	2206.565069	19.400103
49.594678	2198.180009	19.405120
49.761789	2199.765896	19.410138
49.542798	2195.795081	19.415155
49.698232	2192.585538	19.420173
49.617240	2199.927804	19.425191
49.396831	2197.309254	19.430208
49.410228	2194.326509	19.435226
49.661860	2218.398383	19.440243
50.202882	2225.511506	19.445261
49.899542	2221.756571	19.450279
50.172282	2230.434159	19.455296
49.981452	2224.463009	19.460314
49.806216	2218.786106	19.465331
50.386548	2210.993990	19.470349
50.195277	2218.608401	19.475367
50.263910	2223.476978	19.480384
50.660166	2236.706942	19.485402
50.685332	2247.311490	19.490419
51.031416	2235.290173	19.495437
50.721194	2222.663219	19.500455
50.948805	2214.236936	19.505472
51.186302	2212.364090	19.510490
50.916255	2223.230968	19.515507
50.605700	2216.052167	19.520525
50.850448	2210.049786	19.525543
50.569071	2216.714614	19.530560
50.802196	2213.171197	19.535578
50.572446	2233.155335	19.540595
51.049433	2234.587272	19.545613
51.008706	2238.016587	19.550631
50.872956	2243.800357	19.555648
50.951247	2242.011291	19.560666
50.973807	2251.938582	19.565683
50.959683	2235.473284	19.570701
51.017127	2253.468050	19.575719
50.693390	2267.378779	19.580736
51.184326	2273.194615	19.585754
51.367658	2282.579265	19.590771
51.460911	2273.112064	19.595789
51.626615	2277.628625	19.600807
51.628425	2271.948034	19.605824
51.850473	2274.982587	19.610842
51.970162	2277.611655	19.615859
52.097531	2269.721742	19.620877
52.235976	2274.552423	19.625895
52.071637	2263.526372	19.630912
52.407884	2265.456918	19.635930
52.037362	2285.978118	19.640947
52.208213	2265.951447	19.645965
52.511786	2263.642519	19.650983
52.423620	2274.197907	19.656000
52.692335	2268.886360	19.661018
51.824009	2248.950146	19.666035
52.177498	2250.750885	19.671053
52.061134	2260.491710	19.676071
51.777773	2272.074140	19.681088
51.995435	2268.677150	19.686106
52.172793	2271.963750	19.691123
52.496363	2265.351529	19.696141
52.649415	2294.941262	19.701159
52.287642	2302.683881	19.706176
52.476096	2288.839135	19.711194
52.570219	2286.507932	19.716211
53.032778	2290.670548	19.721229
53.120503	2295.800733	19.726247
52.650514	2282.025634	19.731264
52.855113	2288.854846	19.736282
53.205381	2282.142939	19.741299
53.020988	2275.343814	19.746317
53.348053	2285.447360	19.751335
53.144869	2288.141202	19.756352
53.024343	2284.570391	19.761370
53.371263	2282.773343	19.766387
53.445447	2278.436372	19.771405
53.533250	2284.085192	19.776423
53.132918	2283.424526	19.781440
53.411687	2299.082396	19.786458
53.444366	2322.864661	19.791475
53.608961	2317.103417	19.796493
53.818742	2312.572981	19.801511
53.769001	2320.569134	19.806528
53.462948	2315.651542	19.811546
53.701199	2315.830340	19.816563
53.824393	2324.155562	19.821581
54.099353	2308.905882	19.826599
54.023451	2311.563932	19.831616
53.745122	2316.952037	19.836634
54.093226	2315.753751	19.841651
53.820613	2311.364050	19.846669
54.228311	2321.306474	19.851687
54.255508	2331.385595	19.856704
54.161352	2333.153241	19.861722
54.779523	2338.064102	19.866739
54.772276	2331.912192	19.871757
54.935723	2325.978906	19.876775
54.493214	2327.815534	19.881792
54.746790	2328.539782	19.886810
54.582788	2329.598170	19.891827
54.472579	2321.718161	19.896845
54.458563	2314.020471	19.901863
54.526471	2328.761925	19.906880
54.671723	2315.627381	19.911898
55.150873	2312.843410	19.916915
55.044971	2316.459480	19.921933
55.177791	2312.593080	19.926951
55.005920	2309.624789	19.931968
55.482949	2309.098639	19.936986
55.328036	2322.062114	19.942003
55.285830	2319.118846	19.947021
55.513202	2306.918094	19.952039
55.429663	2315.404037	19.957056
55.506952	2304.769877	19.962074
55.255286	2313.454650	19.967091
55.548554	2316.878981	19.972109
55.445163	2312.541819	19.977127
55.437084	2315.306367	19.982144
55.733820	2307.576027	19.987162
55.390008	2307.871680	19.992179
55.395480	2313.867354	19.997197
55.819973	2331.540950	20.002215
55.942974	2349.251595	20.007232
56.192635	2331.509248	20.012250
55.885369	2347.881868	20.017267
55.904191	2355.020329	20.022285
56.382925	2343.143922	20.027303
56.237451	2347.067300	20.032320
56.269777	2341.561348	20.037338
56.138894	2337.412170	20.042355
55.898837	2342.381399	20.047373
56.279545	2342.984845	20.052391
55.884260	2347.905127	20.057408
55.975704	2344.212471	20.062426
56.262417	2360.281849	20.067443
56.119218	2360.758309	20.072461
56.843089	2369.483658	20.077479
56.438923	2375.098072	20.082496
56.658946	2378.499879	20.087514
56.557339	2378.317357	20.092531
56.363974	2380.800161	20.097549
57.233792	2390.881206	20.102567
57.194340	2408.643368	20.107584
56.998896	2404.069643	20.112602
57.156115	2405.022398	20.117619
56.873404	2403.166603	20.122637
57.570945	2406.655436	20.127655
57.323833	2403.809590	20.132672
57.330037	2401.679299	20.137690
57.167513	2410.222634	20.142707
57.048406	2404.657637	20.147725
57.400237	2399.098866	20.152743
57.421685	2410.073990	20.157760
57.545949	2409.287065	20.162778
57.674750	2414.702799	20.167795
57.536877	2432.467081	20.172813
57.559997	2423.205456	20.177831
57.370447	2415.919761	20.182848
57.525374	2422.898765	20.187866
57.831620	2425.165955	20.192883
57.659638	2425.073402	20.197901
57.826151	2439.697101	20.202919
57.952619	2451.519789	20.207936
58.149860	2454.035490	20.212954
58.813141	2447.719781	20.217971
58.513554	2460.104376	20.222989
58.577058	2449.463930	20.228007
58.158618	2454.531367	20.233024
58.292629	2445.515556	20.238042
58.304646	2448.133708	20.243059
58.511751	2444.955336	20.248077
58.748517	2450.744154	20.253095
58.420141	2456.190771	20.258112
58.559895	2447.883202	20.263130
58.976286	2468.275590	20.268147
58.970977	2479.441981	20.273165
58.984557	2477.300225	20.278183
59.242736	2475.685720	20.283200
59.164819	2476.767487	20.288218
59.472743	2473.468126	20.293235
59.367959	2483.519160	20.298253
59.644339	2471.713297	20.303271
59.394194	2455.596584	20.308288
59.207901	2445.605047	20.313306
59.219324	2444.497425	20.318323
59.128030	2468.400787	20.323341
59.414530	2459.442045	20.328359
59.205488	2470.522619	20.333376
59.028530	2474.936624	20.338394
59.416850	2467.047775	20.343411
59.219902	2479.261106	20.348429
59.587027	2489.452844	20.353447
59.547391	2505.421001	20.358464
59.854855	2509.038289	20.363482
60.271584	2500.215471	20.368499
59.864764	2502.661724	20.373517
59.873146	2499.304385	20.378535
59.813824	2503.153333	20.383552
59.921477	2516.371590	20.388570
60.153203	2514.489820	20.393587
60.127002	2536.576176	20.398605
60.441003	2538.265374	20.403623
60.434377	2529.895541	20.408640
60.455117	2523.125395	20.413658
60.656325	2521.708671	20.418675
60.749509	2523.836296	20.423693
60.757179	2526.024308	20.428711
60.464977	2534.072843	20.433728
60.919284	2523.499448	20.438746
60.966357	2524.518834	20.443763
60.895362	2532.975661	20.448781
61.354616	2548.880120	20.453799
61.344924	2554.565818	20.458816
61.291210	2536.678503	20.463834
61.586702	2523.831529	20.468851
61.107683	2524.499107	20.473869
61.474488	2531.354572	20.478887
61.215987	2531.083613	20.483904
61.500496	2549.389600	20.488922
61.671435	2542.161785	20.493939
61.288127	2552.361639	20.498957
61.554721	2545.816977	20.503975
61.566663	2552.377379	20.508992
61.571216	2544.933376	20.514010
61.802754	2542.700086	20.519027
61.905095	2545.946390	20.524045
62.002991	2540.935989	20.529063
61.824821	2541.599124	20.534080
61.871020	2548.568399	20.539098
62.272157	2557.794595	20.544115
61.693544	2572.515571	20.549133
61.902683	2580.775355	20.554151
62.255988	2583.206630	20.559168
62.295513	2576.364859	20.564186
62.328645	2576.336630	20.569203
62.337387	2577.697369	20.574221
62.548143	2570.271045	20.579239
62.662076	2580.675931	20.584256
62.846161	2602.018038	20.589274
62.943116	2598.593682	20.594291
62.893969	2611.266516	20.599309
63.062710	2604.340588	20.604327
63.334580	2598.101704	20.609344
63.181600	2588.985804	20.614362
63.277092	2573.104940	20.619379
63.080582	2570.292823	20.624397
63.038368	2552.525627	20.629415
63.377345	2582.889656	20.634432
62.936516	2601.286632	20.639450
63.317838	2586.152361	20.644467
63.673908	2596.679831	20.649485
63.235524	2586.649552	20.654503
63.387217	2583.862563	20.659520
63.263527	2597.196081	20.664538
63.506297	2587.997659	20.669555
63.608847	2588.696094	20.674573
63.564732	2592.628175	20.679591
63.454310	2590.804315	20.684608
63.675226	2609.772606	20.689626
63.912380	2617.376844	20.694643
63.946586	2618.275733	20.699661
64.128228	2617.323816	20.704679
64.042052	2620.867410	20.709696
63.698141	2615.227092	20.714714
64.046170	2612.898563	20.719731
64.296594	2636.124697	20.724749
64.527943	2639.767193	20.729767
64.576604	2639.497438	20.734784
64.481820	2649.704988	20.739802
64.592723	2641.734147	20.744819
64.807294	2639.377475	20.749837
64.542303	2635.853288	20.754855
65.056826	2630.236844	20.759872
64.934650	2635.213849	20.764890
65.085254	2636.312978	20.769907
64.917669	2631.141906	20.774925
64.734984	2644.701931	20.779943
65.020882	2636.829331	20.784960
65.044037	2638.682146	20.789978
65.197429	2660.279191	20.794995
65.308634	2658.551563	20.800013
65.143162	2671.550538	20.805031
65.599917	2669.728210	20.810048
65.159720	2673.600773	20.815066
65.452342	2669.577572	20.820083
65.575523	2678.573808	20.825101
65.426056	2670.831202	20.830119
65.735407	2670.012103	20.835136
66.031894	2702.240151	20.840154
65.938940	2698.349158	20.845171
65.845762	2705.005533	20.850189
65.915941	2702.278054	20.855207
65.892230	2705.919016	20.860224
65.853624	2699.748128	20.865242
65.955362	2696.576094	20.870259
66.431987	2698.303984	20.875277
66.209502	2711.557673	20.880295
66.044697	2718.918758	20.885312
66.009046	2720.871650	20.890330
66.335467	2720.985100	20.895347
66.662467	2725.806024	20.900365
66.671952	2712.164086	20.905383
66.907384	2716.641697	20.910400
66.645799	2734.429328	20.915418
66.974365	2734.165677	20.920435
67.366141	2746.109698	20.925453
67.418177	2742.483692	20.930471
67.664426	2712.230858	20.935488
67.601719	2714.506309	20.940506
67.867975	2711.998181	20.945523
67.744382	2699.342749	20.950541
67.788276	2695.451779	20.955559
67.937144	2704.607751	20.960576
67.627000	2704.414216	20.965594
68.065690	2694.882981	20.970611
67.787190	2697.463954	20.975629
67.657598	2698.842445	20.980647
67.962090	2693.427604	20.985664
67.552354	2705.209575	20.990682
67.628063	2710.213349	20.995699
67.858111	2692.866717	21.000717
67.577884	2692.960345	21.005735
67.855795	2700.068158	21.010752
67.583559	2705.759307	21.015770
67.974681	2712.635439	21.020787
67.808894	2733.605454	21.025805
67.816171	2728.254282	21.030823
68.425482	2728.642224	21.035840
68.602081	2740.921387	21.040858
68.590177	2735.443469	21.045875
68.443830	2744.662422	21.050893
68.795425	2764.537793	21.055911
68.841203	2762.896552	21.060928
68.859362	2764.185676	21.065946
68.914533	2759.796203	21.070963
68.837586	2768.175013	21.075981
69.070386	2762.768846	21.080999
69.167372	2753.880226	21.086016
68.902650	2761.899535	21.091034
68.962865	2772.517352	21.096051
69.242207	2761.828623	21.101069
69.135388	2779.899964	21.106087
69.407599	2790.383553	21.111104
69.523259	2796.744844	21.116122
69.385679	2797.462893	21.121139
69.536897	2787.270487	21.126157
69.107812	2806.032081	21.131175
69.848491	2798.626735	21.136192
69.547608	2801.302756	21.141210
69.788446	2821.202802	21.146227
70.260380	2831.171948	21.151245
69.882042	2824.719572	21.156263
70.298396	2816.342674	21.161280
70.621836	2813.807956	21.166298
70.772773	2818.397389	21.171315
71.055765	2816.537818	21.176333
70.593851	2818.364520	21.181351
70.673547	2797.552665	21.186368
70.743049	2819.619870	21.191386
70.340608	2808.852840	21.196403
70.498705	2801.957125	21.201421
70.480113	2801.189063	21.206439
70.459193	2806.022233	21.211456
70.437639	2825.692039	21.216474
70.543019	2838.379088	21.221491
70.567799	2836.653912	21.226509
70.407935	2851.834268	21.231527
70.969085	2847.851288	21.236544
71.295315	2860.232190	21.241562
71.547479	2871.108496	21.246579
71.485738	2860.593380	21.251597
71.182910	2863.022502	21.256615
71.272962	2866.235473	21.261632
71.709933	2870.807181	21.266650
71.346295	2863.451622	21.271667
72.136054	2883.139392	21.276685
72.024309	2905.322493	21.281703
72.245388	2903.645969	21.286720
71.972756	2903.227346	21.291738
71.846282	2900.195339	21.296755
71.873038	2897.708452	21.301773
72.015804	2903.036623	21.306791
71.906665	2894.155608	21.311808
72.113988	2896.253990	21.316826
72.252583	2902.161164	21.321843
72.794743	2912.604559	21.326861
72.368039	2912.115732	21.331879
72.587275	2915.943947	21.336896
72.674631	2923.083155	21.341914
72.575722	2920.711908	21.346931
72.890093	2921.876116	21.351949
72.701269	2927.818510	21.356967
73.229076	2912.000694	21.361984
73.156065	2915.848071	21.367002
73.107106	2912.442640	21.372019
73.505961	2901.401801	21.377037
73.426164	2911.223995	21.382055
73.511168	2906.934664	21.387072
73.291735	2904.704589	21.392090
73.233844	2906.856247	21.397107
73.882420	2906.001946	21.402125
73.210684	2911.186777	21.407143
73.663202	2919.645095	21.412160
73.833013	2934.082508	21.417178
73.563023	2946.246272	21.422195
73.708073	2945.562966	21.427213
73.664473	2945.681269	21.432231
73.565551	2937.906358	21.437248
73.812006	2955.525451	21.442266
73.543242	2965.990687	21.447283
74.017151	2970.430736	21.452301
73.971082	2980.351333	21.457319
74.063403	2985.551260	21.462336
74.418015	2998.802344	21.467354
74.577925	2998.733481	21.472371
74.747880	2986.796199	21.477389
74.858072	2997.458664	21.482407
75.514990	2998.330458	21.487424
75.170682	3000.910937	21.492442
75.050161	2992.363621	21.497459
75.161428	2981.620236	21.502477
75.004520	2998.696614	21.507495
74.939080	2980.703641	21.512512
75.609052	2979.980046	21.517530
75.467359	3001.597001	21.522547
75.408810	2991.347791	21.527565
75.132870	2997.527431	21.532583
75.222873	3011.186802	21.537600
75.599796	3017.592802	21.542618
75.496779	3022.400237	21.547635
75.474107	3004.206871	21.552653
75.574229	3031.723396	21.557671
75.622586	3043.882265	21.562688
75.879679	3050.970256	21.567706
75.857272	3061.086592	21.572723
76.230270	3049.676314	21.577741
76.410038	3061.472946	21.582759
76.258388	3057.979733	21.587776
76.371102	3047.755726	21.592794
76.285922	3053.290900	21.597811
76.371685	3071.620507	21.602829
76.773730	3075.058726	21.607847
76.741722	3077.230539	21.612864
76.887377	3087.278964	21.617882
76.779973	3089.641184	21.622899
76.921256	3074.254384	21.627917
76.848862	3081.949175	21.632935
76.980267	3089.823276	21.637952
77.252166	3084.530611	21.642970
76.993928	3075.688696	21.647987
77.638718	3093.831861	21.653005
77.690110	3103.466757	21.658023
77.793744	3094.720932	21.663040
77.587317	3074.689027	21.668058
77.775469	3076.974847	21.673075
77.955409	3071.605653	21.678093
77.731407	3082.190337	21.683111
78.266359	3083.323226	21.688128
78.252631	3072.952781	21.693146
77.918259	3071.317241	21.698163
78.317506	3081.391864	21.703181
78.108737	3079.900916	21.708199
78.304943	3073.174760	21.713216
78.536218	3099.608360	21.718234
78.059759	3101.908737	21.723251
78.582566	3087.629697	21.728269
78.481605	3101.122681	21.733287
78.438773	3096.726080	21.738304
78.923404	3086.059109	21.743322
78.988186	3082.584060	21.748339
78.692734	3089.608658	21.753357
78.591433	3098.831794	21.758375
78.428153	3092.699658	21.763392
78.829838	3106.738693	21.768410
78.507903	3116.086877	21.773427
78.908279	3123.017765	21.778445
79.261728	3133.260614	21.783463
79.059297	3145.453525	21.788480
79.469166	3145.659880	21.793498
79.102387	3147.820884	21.798515
79.584382	3156.623269	21.803533
79.468375	3146.814143	21.808551
79.710929	3168.444210	21.813568
80.180362	3178.258095	21.818586
79.686362	3177.776835	21.823603
79.938698	3182.192933	21.828621
79.723714	3181.341561	21.833639
79.795541	3182.986406	21.838656
79.893514	3185.211162	21.843674
80.031801	3208.500976	21.848691
80.270499	3209.016711	21.853709
80.681349	3215.557340	21.858727
80.684494	3214.552996	21.863744
80.986356	3196.729778	21.868762
81.051562	3206.014435	21.873779
80.993951	3217.787423	21.878797
81.114948	3206.343873	21.883815
81.053417	3209.540233	21.888832
81.114269	3212.182531	21.893850
81.168156	3210.382427	21.898867
81.283686	3221.418562	21.903885
81.512969	3237.477873	21.908903
81.309910	3232.753391	21.913920
81.456434	3228.412468	21.918938
81.490172	3233.693023	21.923955
81.428007	3226.684309	21.928973
81.679744	3228.662016	21.933991
81.484347	3232.266711	21.939008
81.937040	3236.825301	21.944026
81.988368	3259.798864	21.949043
82.119840	3260.240196	21.954061
82.133701	3260.067518	21.959079
82.026848	3251.699684	21.964096
82.279263	3254.405606	21.969114
82.109055	3265.942913	21.974131
82.423995	3262.921354	21.979149
82.582902	3257.047320	21.984167
82.392966	3272.475176	21.989184
82.354487	3270.254120	21.994202
82.580506	3276.585168	21.999219
82.798248	3288.281606	22.004237
82.970662	3292.090881	22.009255
82.620149	3285.865596	22.014272
82.745488	3282.359236	22.019290
82.920332	3308.167890	22.024307
82.873892	3312.745600	22.029325
83.073575	3303.949928	22.034343
82.823396	3319.253143	22.039360
83.386006	3334.494107	22.044378
83.341130	3339.094400	22.049395
83.487392	3337.066423	22.054413
83.555688	3340.873625	22.059431
83.599077	3336.637114	22.064448
83.638226	3332.602874	22.069466
83.863268	3360.198155	22.074483
83.778655	3376.673251	22.079501
84.234018	3370.016738	22.084519
84.208776	3377.249170	22.089536
84.517369	3358.967971	22.094554
84.313070	3364.569789	22.099571
84.369239	3350.859340	22.104589
84.920120	3366.334552	22.109607
84.911849	3368.589489	22.114624
85.043592	3379.789195	22.119642
85.219624	3387.212776	22.124659
85.045201	3371.634156	22.129677
85.404072	3370.171816	22.134695
85.136200	3383.565465	22.139712
85.669265	3376.587848	22.144730
85.614629	3383.851124	22.149747
85.672365	3379.252002	22.154765
85.586016	3364.060007	22.159783
85.516760	3370.026510	22.164800
85.782223	3374.347190	22.169818
85.727326	3378.496011	22.174835
85.737272	3371.653264	22.179853
85.825632	3377.123263	22.184871
85.811072	3378.059979	22.189888
85.973525	3370.327878	22.194906
86.023025	3376.612941	22.199923
86.258013	3400.946884	22.204941
86.432956	3402.206217	22.209959
86.312524	3404.677327	22.214976
86.532552	3407.333511	22.219994
86.605579	3407.323886	22.225011
86.120272	3413.741432	22.230029
86.507253	3407.019040	22.235047
86.685390	3419.869736	22.240064
86.807180	3428.125905	22.245082
86.794722	3436.884176	22.250099
86.989257	3430.632149	22.255117
87.042658	3437.388236	22.260135
86.916244	3451.953033	22.265152
87.461826	3458.400637	22.270170
87.400165	3468.491048	22.275187
87.482354	3479.324612	22.280205
87.811793	3457.222592	22.285223
87.567638	3461.632626	22.290240
87.784937	3454.389838	22.295258
87.808213	3464.198105	22.300275
87.858198	3463.528519	22.305293
88.014241	3464.553976	22.310311
88.256284	3487.136525	22.315328
88.376671	3482.206945	22.320346
88.679889	3491.382366	22.325363
88.831594	3491.483753	22.330381
89.138677	3472.629450	22.335399
88.494735	3467.674606	22.340416
88.649563	3468.785696	22.345434
88.936080	3474.552113	22.350451
89.028631	3485.480424	22.355469
89.033966	3493.758628	22.360487
89.041867	3482.836705	22.365504
89.008900	3487.894516	22.370522
89.008034	3484.671954	22.375539
88.930862	3481.096654	22.380557
88.979878	3481.735080	22.385575
88.876603	3496.811836	22.390592
89.031562	3497.885111	22.395610
89.369663	3514.346407	22.400627
89.027411	3515.843967	22.405645
89.327619	3520.010129	22.410663
89.449344	3540.013459	22.415680
89.673226	3540.984011	22.420698
90.016650	3538.056510	22.425715
89.901749	3550.488815	22.430733
90.380855	3569.298495	22.435751
90.028127	3572.628088	22.440768
90.383896	3575.244548	22.445786
90.665631	3573.903990	22.450803
90.239726	3576.920877	22.455821
90.477435	3575.607279	22.460839
90.303534	3594.801271	22.465856
90.883445	3590.248869	22.470874
91.199191	3595.923101	22.475891
90.904858	3604.409543	22.480909
91.542768	3588.872846	22.485927
91.610888	3590.876218	22.490944
91.608647	3599.148644	22.495962
91.652701	3591.036002	22.500979
91.471576	3590.067202	22.505997
91.828936	3590.757041	22.511015
91.671100	3587.841891	22.516032
91.783094	3591.007293	22.521050
92.215901	3611.858910	22.526067
92.016961	3619.218188	22.531085
92.252663	3617.758856	22.536103
92.354845	3619.998728	22.541120
92.466602	3624.481096	22.546138
92.661312	3610.475086	22.551155
92.468200	3623.998711	22.556173
92.677262	3614.408013	22.561191
92.733259	3611.810276	22.566208
92.783175	3608.376149	22.571226
93.025117	3609.268525	22.576243
92.775032	3613.239821	22.581261
92.859858	3603.810996	22.586279
93.215768	3633.023315	22.591296
92.926383	3648.045538	22.596314
93.139312	3638.021511	22.601331
93.108001	3639.133451	22.606349
93.396843	3645.058602	22.611367
93.333492	3644.943560	22.616384
93.041134	3662.237536	22.621402
93.404712	3669.782230	22.626419
93.412935	3667.145921	22.631437
93.333796	3671.651187	22.636455
94.042843	3685.533660	22.641472
94.042268	3694.792079	22.646490
94.030641	3698.463364	22.651507
94.186479	3699.168793	22.656525
94.333288	3695.847769	22.661543
94.404875	3715.413155	22.666560
94.349083	3726.657094	22.671578
94.368255	3725.617391	22.676595
94.156426	3740.376888	22.681613
94.739463	3734.777864	22.686631
94.752317	3734.536450	22.691648
95.004534	3748.261004	22.696666
95.333837	3765.629534	22.701683
95.275403	3757.586103	22.706701
95.740486	3748.373489	22.711719
95.830934	3746.700353	22.716736
95.496542	3746.476949	22.721754
95.896546	3747.812112	22.726771
95.670925	3757.784135	22.731789
96.123750	3744.333385	22.736807
96.110323	3736.054575	22.741824
95.912110	3746.133873	22.746842
96.208187	3739.029903	22.751859
96.148915	3750.282701	22.756877
96.388234	3744.308976	22.761895
96.159189	3750.852424	22.766912
96.292718	3762.709199	22.771930
96.615324	3773.159146	22.776947
96.281737	3788.943141	22.781965
96.450758	3772.550276	22.786983
96.326046	3782.930839	22.792000
96.540459	3798.740826	22.797018
96.718418	3799.593786	22.802035
96.775159	3817.565684	22.807053
96.862792	3813.298897	22.812071
97.286659	3820.278580	22.817088
97.171382	3826.413494	22.822106
97.291499	3851.256105	22.827123
97.173605	3850.349281	22.832141
97.613707	3851.875861	22.837159
97.735459	3869.933140	22.842176
97.450637	3870.214145	22.847194
98.028256	3863.111234	22.852211
98.053265	3867.424935	22.857229
98.326329	3869.192901	22.862247
98.350617	3873.003569	22.867264
98.146730	3892.633596	22.872282
98.712260	3903.530108	22.877299
98.487107	3901.778790	22.882317
98.443569	3893.976531	22.887335
98.637760	3897.996927	22.892352
98.354001	3913.254305	22.897370
98.691996	3913.635939	22.902387
98.971045	3924.840438	22.907405
98.698956	3933.583229	22.912423
99.369985	3946.876543	22.917440
99.522863	3964.678785	22.922458
99.842567	3957.679475	22.927475
99.653281	3966.509390	22.932493
99.646967	3970.265295	22.937511
99.882198	3960.922032	22.942528
99.680170	3963.853571	22.947546
99.845443	3952.025773	22.952563
99.873583	3969.783671	22.957581
100.113734	3973.883502	22.962599
100.448844	3988.211904	22.967616
100.267230	3982.546231	22.972634
100.325048	3976.076023	22.977651
100.521981	3970.201737	22.982669
100.598643	3987.185484	22.987687
101.004540	4007.848376	22.992704
101.325980	4006.998081	22.997722
101.358126	4008.475946	23.002739
101.427621	4001.861669	23.007757
101.344233	4007.215780	23.012775
101.511677	3997.047462	23.017792
101.407734	4006.584963	23.022810
101.832386	3995.004040	23.027827
101.648539	4010.905645	23.032845
101.478435	4006.143590	23.037863
101.766361	4005.980341	23.042880
101.530021	4004.263932	23.047898
102.179066	4007.490678	23.052915
101.707825	4009.918276	23.057933
101.949056	4034.082098	23.062951
101.985921	4032.557946	23.067968
101.939378	4043.824208	23.072986
101.886365	4039.208939	23.078003
102.335215	4055.895428	23.083021
102.605584	4074.040199	23.088039
102.782240	4068.582622	23.093056
102.508936	4070.383020	23.098074
103.210498	4070.300636	23.103091
103.081235	4073.690260	23.108109
102.906190	4076.572478	23.113127
103.513345	4080.422317	23.118144
103.111169	4089.233542	23.123162
103.241534	4078.455535	23.128179
103.281094	4093.109256	23.133197
103.408752	4103.182969	23.138215
103.568963	4108.762222	23.143232
103.291257	4118.985607	23.148250
103.700883	4123.479531	23.153267
103.850764	4140.403314	23.158285
103.978709	4136.323483	23.163303
104.622917	4136.684446	23.168320
104.391991	4139.201097	23.173338
104.650009	4151.497059	23.178355
104.922421	4168.465981	23.183373
104.999933	4168.372147	23.188391
105.465474	4166.325165	23.193408
105.521603	4164.808841	23.198426
105.542503	4154.770937	23.203443
105.799795	4156.204920	23.208461
105.461676	4148.196872	23.213479
105.991957	4133.889659	23.218496
105.529505	4143.723105	23.223514
105.511899	4146.561210	23.228531
105.545946	4154.890928	23.233549
105.523420	4157.366451	23.238567
105.735586	4148.681630	23.243584
105.982409	4160.233760	23.248602
105.570289	4181.710816	23.253619
106.009952	4183.456407	23.258637
105.928589	4196.428582	23.263655
106.167133	4197.233364	23.268672
106.122054	4210.267668	23.273690
106.290839	4215.304975	23.278707
106.443421	4222.556842	23.283725
106.700324	4235.749540	23.288743
106.851041	4240.881970	23.293760
106.681481	4253.475447	23.298778
107.235312	4245.130191	23.303795
107.187842	4255.406175	23.308813
107.370020	4271.102281	23.313831
107.695901	4279.973627	23.318848
107.822340	4284.719912	23.323866
107.741183	4268.342275	23.328883
107.812341	4271.816150	23.333901
108.074011	4281.776492	23.338919
108.121262	4271.697937	23.343936
107.960859	4282.379621	23.348954
107.836859	4302.677303	23.353971
108.759220	4298.008267	23.358989
108.043252	4300.283428	23.364007
108.600833	4299.346458	23.369024
108.392751	4299.468326	23.374042
108.588047	4305.660773	23.379059
108.710116	4323.411429	23.384077
109.086288	4333.782427	23.389095
109.085297	4319.263610	23.394112
109.082735	4330.416114	23.399130
109.210020	4330.053809	23.404147
109.354806	4323.915950	23.409165
109.407983	4361.174852	23.414183
109.728028	4359.590882	23.419200
109.625656	4346.478611	23.424218
109.901713	4358.896172	23.429235
109.689046	4348.891620	23.434253
109.836939	4359.743289	23.439271
110.106985	4384.300942	23.444288
110.278251	4383.829002	23.449306
110.013078	4396.584462	23.454323
110.535338	4394.769428	23.459341
110.383713	4398.849461	23.464359
110.530726	4409.439093	23.469376
110.695973	4423.832976	23.474394
110.740881	4437.406168	23.479411
110.764603	4432.346587	23.484429
110.717487	4449.582404	23.489447
111.147615	4452.714706	23.494464
111.006361	4456.076472	23.499482
111.334720	4473.010890	23.504499
111.468056	4480.712535	23.509517
111.560815	4490.387915	23.514535
111.887287	4488.803658	23.519552
112.049814	4494.078322	23.524570
112.144286	4509.134798	23.529587
112.165433	4516.433325	23.534605
112.398363	4514.749556	23.539623
112.752974	4513.608307	23.544640
112.575541	4518.020211	23.549658
112.940856	4508.479133	23.554675
113.146219	4516.976415	23.559693
112.853321	4520.837686	23.564711
112.970679	4502.815106	23.569728
113.185590	4509.289841	23.574746
113.387257	4520.355581	23.579763
113.772364	4528.852698	23.584781
113.520425	4532.556015	23.589799
113.966489	4527.826241	23.594816
114.264391	4527.578659	23.599834
113.572545	4534.909574	23.604851
113.836261	4528.541735	23.609869
113.736292	4536.992627	23.614887
114.022517	4543.906403	23.619904
114.362685	4550.295492	23.624922
114.083148	4557.203544	23.629939
114.153240	4574.580770	23.634957
113.994737	4579.663616	23.639975
114.035470	4581.377531	23.644992
114.377469	4596.001435	23.650010
114.243346	4610.411099	23.655027
114.839970	4610.337002	23.660045
114.948540	4632.753497	23.665063
115.075285	4623.004906	23.670080
115.191339	4639.507631	23.675098
115.226932	4652.838047	23.680115
115.249332	4647.389222	23.685133
115.286842	4660.687042	23.690151
115.504318	4682.585583	23.695168
116.064069	4684.620070	23.700186
116.398790	4691.132173	23.705203
116.279033	4678.667417	23.710221
116.015604	4689.723119	23.715239
116.390711	4680.355132	23.720256
116.849888	4686.879741	23.725274
116.867642	4707.456118	23.730291
117.130797	4700.511494	23.735309
117.180706	4703.799202	23.740327
117.173891	4694.911271	23.745344
117.451878	4707.296506	23.750362
117.501954	4710.171170	23.755379
117.481069	4702.658875	23.760397
117.110737	4709.438680	23.765415
117.301286	4699.546026	23.770432
117.946402	4694.461244	23.775450
117.517437	4701.370426	23.780467
117.661193	4729.669410	23.785485
117.965349	4734.153774	23.790503
117.915291	4728.882652	23.795520
117.778873	4735.757289	23.800538
118.016515	4745.135247	23.805555
118.658169	4745.299395	23.810573
118.451554	4759.294375	23.815591
118.998306	4757.904417	23.820608
119.140955	4752.781770	23.825626
119.004582	4757.035371	23.830643
119.085085	4784.647617	23.835661
118.978828	4781.720173	23.840679
119.348320	4788.369101	23.845696
119.728008	4789.461637	23.850714
119.698007	4786.346383	23.855731
119.643998	4793.761403	23.860749
119.577149	4802.123102	23.865767
119.824435	4817.792858	23.870784
120.414190	4811.723022	23.875802
120.232975	4819.778409	23.880819
120.457139	4817.512945	23.885837
120.040342	4820.015925	23.890855
120.195296	4849.540921	23.895872
120.622942	4840.675611	23.900890
120.303303	4848.976343	23.905907
120.631410	4862.810217	23.910925
120.641329	4877.230186	23.915943
120.959835	4871.946936	23.920960
120.873222	4882.173497	23.925978
121.284559	4911.583011	23.930995
121.632145	4900.852408	23.936013
121.891320	4904.096523	23.941031
121.703802	4911.169459	23.946048
122.240641	4902.957383	23.951066
122.041114	4907.322649	23.956083
122.372964	4910.544913	23.961101
122.479137	4928.145722	23.966119
122.619058	4930.033065	23.971136
122.582529	4930.107689	23.976154
122.882793	4933.643075	23.981171
123.097867	4929.997889	23.986189
123.174530	4925.460937	23.991207
122.904686	4930.423700	23.996224
122.961338	4932.272830	24.001242
123.221741	4938.925280	24.006259
123.172680	4949.212220	24.011277
123.463944	4958.726734	24.016295
123.291677	4964.706536	24.021312
123.543086	4958.662236	24.026330
123.869812	4975.237207	24.031347
123.954503	4989.647286	24.036365
123.714040	4980.087902	24.041383
123.922429	4981.628477	24.046400
124.069112	4989.067124	24.051418
124.055842	5016.924428	24.056435
124.338171	5004.398089	24.061453
124.660253	5004.239428	24.066471
124.543045	5007.207935	24.071488
124.698327	5023.478582	24.076506
124.691713	5036.144590	24.081523
124.879916	5028.861784	24.086541
125.103516	5046.127548	24.091559
125.115133	5068.984348	24.096576
125.543797	5063.861587	24.101594
125.529964	5077.093830	24.106611
125.181213	5069.816260	24.111629
125.598256	5085.173170	24.116647
125.712960	5095.116976	24.121664
126.115624	5098.435068	24.126682
126.035442	5107.529906	24.131699
126.174490	5114.413920	24.136717
126.660440	5128.760973	24.141735
126.398437	5133.642576	24.146752
127.090158	5122.137571	24.151770
127.180067	5139.814935	24.156787
127.327964	5148.451598	24.161805
127.499277	5156.711134	24.166823
127.400678	5155.415181	24.171840
127.525691	5163.304384	24.176858
127.492597	5154.342181	24.181875
127.657510	5151.079676	24.186893
127.948906	5160.884081	24.191911
127.600293	5177.324380	24.196928
127.971097	5168.131634	24.201946
127.880200	5192.183221	24.206963
128.078228	5189.484975	24.211981
128.511409	5206.887168	24.216999
128.211383	5214.806075	24.222016
128.425237	5216.370576	24.227034
128.390444	5238.225747	24.232051
128.478523	5245.911626	24.237069
128.620445	5255.465566	24.242087
128.808490	5279.701926	24.247104
129.150808	5276.816420	24.252122
128.985507	5292.338272	24.257139
129.223357	5320.730269	24.262157
129.754584	5310.048579	24.267175
129.745495	5308.912643	24.272192
130.052846	5318.484173	24.277210
130.022631	5340.900599	24.282227
130.303888	5345.651944	24.287245
130.489138	5337.745796	24.292263
130.528225	5348.341695	24.297280
130.371703	5336.039592	24.302298
130.879618	5362.599061	24.307315
131.432697	5368.597365	24.312333
131.262956	5354.462988	24.317351
131.413985	5364.263941	24.322368
131.529669	5363.793283	24.327386
131.647770	5363.809678	24.332403
131.749468	5363.149972	24.337421
131.660283	5381.732885	24.342439
131.524597	5389.716861	24.347456
132.066648	5392.003609	24.352474
131.804610	5395.170549	24.357491
131.950291	5401.267684	24.362509
132.295994	5418.155377	24.367527
132.537618	5427.434259	24.372544
132.773332	5427.638329	24.377562
132.763918	5432.420800	24.382579
132.698939	5440.335631	24.387597
133.040688	5441.197057	24.392615
132.756075	5450.164045	24.397632
133.087834	5441.589470	24.402650
133.116565	5465.802438	24.407667
133.193848	5465.757067	24.412685
133.686590	5474.630268	24.417703
133.510475	5482.915099	24.422720
133.508220	5483.232122	24.427738
133.948254	5505.431300	24.432755
133.878096	5514.012060	24.437773
134.014186	5505.124862	24.442791
134.317671	5545.296350	24.447808
134.656125	5539.667415	24.452826
134.978251	5543.939179	24.457843
134.516945	5548.404971	24.462861
134.650177	5553.421813	24.467879
134.764612	5569.846251	24.472896
135.085514	5561.293881	24.477914
135.109632	5577.817907	24.482931
135.315155	5599.517323	24.487949
135.826565	5603.253041	24.492967
135.894087	5604.595669	24.497984
135.978820	5602.358646	24.503002
136.269499	5611.996899	24.508019
136.246613	5636.871495	24.513037
136.454825	5624.501810	24.518055
136.258727	5634.177985	24.523072
136.581138	5622.544642	24.528090
136.793138	5643.210639	24.533107
136.997030	5657.651250	24.538125
137.341234	5645.073227	24.543143
137.367306	5659.435335	24.548160
137.422244	5656.229485	24.553178
137.627182	5655.204634	24.558195
137.900021	5669.698438	24.563213
138.171783	5678.005046	24.568231
137.942758	5691.613172	24.573248
138.057288	5680.133442	24.578266
138.082245	5677.675155	24.583283
137.972969	5684.568559	24.588301
138.288618	5691.642572	24.593319
138.529238	5712.668939	24.598336
138.134713	5710.559130	24.603354
138.464937	5726.506289	24.608371
138.351392	5737.315884	24.613389
138.887474	5760.329582	24.618407
138.728119	5773.369501	24.623424
139.101415	5785.649675	24.628442
139.336065	5800.405850	24.633459
139.155810	5806.337285	24.638477
139.780478	5813.533150	24.643495
139.547003	5830.687880	24.648512
139.887098	5834.077109	24.653530
140.094828	5845.581037	24.658547
140.269024	5842.154629	24.663565
140.874436	5844.064392	24.668583
140.905017	5858.138102	24.673600
141.096975	5872.797842	24.678618
141.498774	5871.899919	24.683635
141.302143	5879.820974	24.688653
141.475222	5866.758777	24.693671
141.455815	5874.713547	24.698688
141.721123	5872.382465	24.703706
141.722986	5888.640775	24.708723
141.934324	5904.416394	24.713741
142.169249	5897.538910	24.718759
141.824662	5903.845222	24.723776
141.703627	5914.350622	24.728794
142.142675	5908.876612	24.733811
142.136092	5923.250657	24.738829
142.485519	5927.985798	24.743847
142.379426	5933.562853	24.748864
142.269928	5945.097221	24.753882
142.845788	5955.573728	24.758899
142.720032	5964.135177	24.763917
142.994485	5972.046952	24.768935
142.919625	5982.959394	24.773952
142.935415	6003.009376	24.778970
143.931021	6010.844928	24.783987
144.412272	6015.955222	24.789005
145.038881	5987.847296	24.794023
145.010129	5988.419138	24.799040
145.074336	5976.597456	24.804058
145.406324	5986.064130	24.809075
145.187296	5993.446346	24.814093
145.445425	5982.055282	24.819111
145.383097	5984.669580	24.824128
145.464203	5986.340359	24.829146
145.251901	5974.436397	24.834163
145.203413	5987.516845	24.839181
145.566006	5985.876468	24.844199
145.596978	5978.296322	24.849216
145.895563	5997.683338	24.854234
145.960818	6006.773959	24.859251
146.001415	6019.875545	24.864269
145.835113	6023.006709	24.869287
146.192571	6031.384397	24.874304
146.342555	6041.832106	24.879322
146.495014	6046.932950	24.884339
146.163809	6059.599869	24.889357
146.542004	6079.642829	24.894375
146.623545	6087.516450	24.899392
146.869137	6105.496000	24.904410
147.290625	6117.393613	24.909427
147.118712	6120.885621	24.914445
147.391641	6140.691683	24.919463
147.654951	6144.754400	24.924480
147.343270	6157.994639	24.929498
147.602014	6170.252305	24.934515
147.769068	6188.507961	24.939533
147.997755	6200.349292	24.944551
148.187542	6218.950889	24.949568
148.276701	6226.612263	24.954586
148.951376	6235.805500	24.959603
148.439559	6258.341010	24.964621
148.917369	6264.535594	24.969639
149.148923	6266.770222	24.974656
149.276838	6284.808012	24.979674
149.451472	6294.135098	24.984691
149.378117	6313.296120	24.989709
149.749385	6302.196025	24.994727
150.082544	6326.498624	24.999744
150.296006	6339.551437	25.004762
150.478431	6331.810640	25.009779
150.322076	6337.735175	25.014797
150.848914	6352.155353	25.019815
150.994045	6360.069793	25.024832
151.442469	6362.129206	25.029850
151.564666	6368.247137	25.034867
151.370368	6371.500338	25.039885
151.619195	6365.281882	25.044903
152.055834	6362.060463	25.049920
151.620290	6359.815585	25.054938
152.468649	6372.050013	25.059955
152.067686	6388.581341	25.064973
151.979188	6382.331200	25.069991
152.297069	6394.042959	25.075008
152.266340	6389.948206	25.080026
152.936866	6397.631731	25.085043
152.691813	6418.738903	25.090061
152.966147	6410.260709	25.095079
152.749176	6415.788133	25.100096
152.637728	6435.215485	25.105114
152.776184	6447.340462	25.110131
152.981578	6453.153290	25.115149
153.373807	6473.660658	25.120167
153.385210	6493.816733	25.125184
153.435126	6488.812408	25.130202
154.022428	6503.393630	25.135219
153.819045	6526.471576	25.140237
154.093300	6543.170286	25.145255
154.227503	6540.038183	25.150272
154.450435	6554.548928	25.155290
155.278934	6564.820292	25.160307
155.504008	6565.555762	25.165325
155.223648	6573.926513	25.170343
155.487176	6572.251256	25.175360
155.561740	6579.532468	25.180378
155.531907	6589.558203	25.185395
155.861373	6601.760419	25.190413
155.688904	6607.198652	25.195431
156.122110	6602.332568	25.200448
155.966811	6635.056472	25.205466
156.476509	6640.845076	25.210483
156.367218	6642.317816	25.215501
156.692655	6654.562479	25.220519
156.849702	6672.198188	25.225536
156.879726	6670.523701	25.230554
157.112348	6679.615408	25.235571
157.362471	6697.936686	25.240589
157.428761	6700.041961	25.245607
157.781406	6706.173924	25.250624
157.808398	6739.735018	25.255642
158.103766	6722.379037	25.260659
157.941546	6736.542488	25.265677
158.103292	6748.175566	25.270695
158.716415	6753.981776	25.275712
158.389196	6766.477703	25.280730
158.521835	6766.837042	25.285747
158.617226	6787.407257	25.290765
158.964355	6802.380481	25.295783
159.491251	6804.148982	25.300800
159.045616	6822.589306	25.305818
159.783133	6826.322615	25.310835
159.703815	6836.159006	25.315853
159.884205	6846.677045	25.320871
159.825603	6862.788447	25.325888
160.097930	6866.464746	25.330906
160.527876	6876.609219	25.335923
160.720294	6876.245942	25.340941
160.739919	6883.945116	25.345959
161.232479	6880.772634	25.350976
160.608392	6897.971411	25.355994
161.077824	6902.391685	25.361011
161.481414	6915.289915	25.366029
161.767687	6927.524723	25.371047
162.307045	6933.563707	25.376064
162.168140	6942.557080	25.381082
162.400843	6932.226049	25.386099
162.396066	6944.821625	25.391117
162.156566	6924.780003	25.396135
162.788822	6936.090544	25.401152
162.827338	6955.065323	25.406170
162.949696	6954.251320	25.411187
163.066420	6967.240309	25.416205
162.749186	6964.114985	25.421223
163.103375	6963.456416	25.426240
162.941798	6990.681747	25.431258
163.440382	6992.436835	25.436275
163.477985	7009.443703	25.441293
163.749403	7019.772765	25.446311
163.731070	7023.543595	25.451328
163.883202	7038.581555	25.456346
164.013964	7057.750708	25.461363
164.195626	7070.019452	25.466381
164.644013	7080.967482	25.471399
164.655588	7087.778132	25.476416
164.514432	7118.531775	25.481434
164.986874	7121.919108	25.486451
164.965838	7127.231688	25.491469
164.965610	7154.640136	25.496487
165.468529	7166.273855	25.501504
165.705739	7176.092023	25.506522
166.092226	7183.321974	25.511539
166.194814	7189.964052	25.516557
166.441405	7203.444489	25.521575
166.850474	7217.317869	25.526592
166.672082	7225.009762	25.531610
166.798413	7220.415507	25.536627
166.872286	7242.636696	25.541645
166.808840	7261.614514	25.546663
167.420217	7260.540914	25.551680
167.428861	7290.944870	25.556698
167.894566	7296.891417	25.561715
168.129645	7299.570595	25.566733
168.159621	7313.772114	25.571751
168.352357	7314.057743	25.576768
168.263820	7314.556027	25.581786
168.167745	7333.017944	25.586803
168.456839	7350.890133	25.591821
168.540562	7355.475080	25.596839
168.883792	7365.216779	25.601856
169.057860	7375.434571	25.606874
169.000260	7408.217967	25.611891
169.578267	7419.412595	25.616909
169.431579	7420.878985	25.621927
169.620183	7429.660214	25.626944
169.749630	7449.393186	25.631962
170.195890	7470.768727	25.636979
170.456913	7479.149736	25.641997
170.321083	7490.016589	25.647015
170.980161	7502.710055	25.652032
170.993701	7504.950169	25.657050
171.018993	7516.833189	25.662067
171.017505	7532.106502	25.667085
171.203367	7545.684688	25.672103
171.460307	7558.339109	25.677120
171.204892	7579.307774	25.682138
171.650045	7581.457680	25.687156
172.132597	7599.881795	25.692173
171.928373	7624.043639	25.697191
172.521496	7630.385110	25.702208
172.446764	7642.840795	25.707226
172.933697	7653.833263	25.712244
173.066175	7657.487176	25.717261
173.252484	7685.234318	25.722279
173.510747	7682.801357	25.727296
173.629704	7688.907736	25.732314
173.880599	7697.162944	25.737332
174.287894	7692.366183	25.742349
174.158076	7706.729138	25.747367
174.277021	7698.010510	25.752384
174.190559	7709.723903	25.757402
174.428235	7740.721750	25.762420
174.766735	7737.858094	25.767437
174.645413	7746.050389	25.772455
175.238467	7766.717649	25.777472
175.353643	7774.085640	25.782490
175.177548	7772.378148	25.787508
175.771077	7776.846689	25.792525
175.737809	7799.893660	25.797543
176.232819	7807.599009	25.802560
176.058384	7811.994401	25.807578
176.066858	7810.418655	25.812596
176.097471	7818.711112	25.817613
176.096268	7847.438588	25.822631
176.602475	7859.727569	25.827648
176.668088	7869.413850	25.832666
176.588434	7874.961624	25.837684
177.435049	7889.394963	25.842701
177.382125	7894.341317	25.847719
177.365464	7922.550085	25.852736
177.559726	7931.711076	25.857754
177.621154	7949.495544	25.862772
178.038428	7960.076788	25.867789
178.064713	7987.375970	25.872807
178.481631	7986.051703	25.877824
178.281614	8011.008933	25.882842
178.699715	8019.701376	25.887860
179.083970	8024.455029	25.892877
178.936302	8042.396232	25.897895
179.126123	8053.819279	25.902912
179.485398	8067.374774	25.907930
179.649215	8094.578955	25.912948
180.063368	8086.914793	25.917965
179.924882	8127.970456	25.922983
180.547504	8128.286673	25.928000
180.476498	8125.993903	25.933018
180.541102	8151.416434	25.938036
180.807788	8153.636078	25.943053
180.906333	8176.154586	25.948071
181.460417	8198.282807	25.953088
181.859251	8197.397068	25.958106
181.652708	8200.314773	25.963124
182.236534	8204.197472	25.968141
182.049945	8229.871930	25.973159
182.052585	8218.621110	25.978176
182.750167	8238.327353	25.983194
182.947067	8254.832726	25.988212
183.081376	8256.842695	25.993229
183.276851	8254.918592	25.998247
183.782299	8265.679229	26.003264
183.616761	8279.565788	26.008282
183.425938	8283.082659	26.013300
183.882113	8281.831433	26.018317
183.792556	8300.940832	26.023335
183.813508	8311.902062	26.028352
184.128494	8318.040880	26.033370
184.771418	8337.098606	26.038388
185.272045	8334.100938	26.043405
185.358219	8347.115801	26.048423
185.735037	8330.920538	26.053440
185.959370	8327.574708	26.058458
185.919725	8331.710106	26.063476
185.874274	8319.903215	26.068493
185.812652	8349.038550	26.073511
186.220529	8365.270526	26.078528
186.250137	8356.415072	26.083546
186.257990	8371.582109	26.088564
186.509461	8372.767772	26.093581
186.239554	8382.141193	26.098599
186.834638	8390.857370	26.103616
187.191557	8396.516709	26.108634
187.011540	8418.290015	26.113652
187.609170	8420.280948	26.118669
187.227844	8428.160543	26.123687
187.286133	8434.426886	26.128704
188.035268	8442.295345	26.133722
188.347431	8452.242911	26.138740
188.591517	8456.323584	26.143757
188.679618	8476.797174	26.148775
188.670214	8476.611349	26.153792
189.329385	8479.858646	26.158810
188.821547	8486.444603	26.163828
189.179344	8501.952488	26.168845
189.147539	8527.567984	26.173863
189.294065	8542.997398	26.178880
189.214216	8553.778540	26.183898
189.063659	8579.276690	26.188916
189.492409	8586.082854	26.193933
189.770910	8619.266117	26.198951
189.890459	8632.313506	26.203968
190.324646	8632.481290	26.208986
190.954167	8668.691872	26.214004
191.504283	8670.867910	26.219021
191.678801	8675.012908	26.224039
191.490602	8695.450516	26.229056
192.254540	8706.936705	26.234074
192.024154	8701.268321	26.239092
192.463706	8701.615591	26.244109
192.706088	8710.681654	26.249127
192.476626	8732.981835	26.254144
192.621216	8733.151787	26.259162
192.943841	8744.342299	26.264180
193.302415	8757.090372	26.269197
193.132102	8768.301699	26.274215
193.238146	8777.076842	26.279232
193.769801	8802.764300	26.284250
193.477727	8808.355373	26.289268
193.863545	8826.596052	26.294285
194.412491	8835.187774	26.299303
193.826977	8857.763566	26.304320
194.550816	8857.714148	26.309338
194.564692	8883.390408	26.314356
194.551434	8895.749488	26.319373
195.028649	8906.879128	26.324391
195.355383	8922.704472	26.329408
195.719665	8929.048052	26.334426
195.514141	8936.621593	26.339444
195.910156	8941.175092	26.344461
196.642116	8969.218705	26.349479
196.676929	8983.126335	26.354496
196.877946	8976.820241	26.359514
196.586766	8998.607194	26.364532
196.875827	9010.222479	26.369549
196.942806	9017.373740	26.374567
197.071513	9040.977047	26.379584
197.657701	9047.429728	26.384602
197.906994	9062.157396	26.389620
197.954983	9078.927683	26.394637
197.972712	9089.668647	26.399655
198.287610	9101.088325	26.404672
198.664071	9115.645373	26.409690
198.675901	9122.075623	26.414708
198.699872	9140.917581	26.419725
198.434810	9160.000299	26.424743
198.856980	9178.728460	26.429760
199.637686	9184.496076	26.434778
199.598564	9210.340731	26.439796
199.631075	9220.872970	26.444813
199.936178	9234.529789	26.449831
199.934422	9247.496903	26.454848
200.196539	9272.330919	26.459866
200.268270	9287.928588	26.464884
200.551773	9283.870960	26.469901
200.878446	9311.619024	26.474919
201.412524	9332.557226	26.479936
201.315604	9330.884530	26.484954
201.627147	9348.037690	26.489972
201.560406	9363.053372	26.494989
202.007143	9374.421531	26.500007
201.900704	9398.345424	26.505024
202.264846	9406.518225	26.510042
202.107748	9429.140614	26.515060
202.446281	9435.251559	26.520077
202.746563	9455.422749	26.525095
203.060425	9476.088753	26.530112
203.654677	9485.680798	26.535130
203.680836	9505.837481	26.540148
203.663232	9525.259415	26.545165
204.273763	9533.813773	26.550183
204.216071	9543.738066	26.555200
204.732776	9540.891910	26.560218
205.156677	9543.454417	26.565236
205.383577	9560.361853	26.570253
205.759873	9572.800454	26.575271
205.372249	9588.723227	26.580288
205.728279	9591.640391	26.585306
205.804800	9602.058484	26.590324
205.971213	9608.131769	26.595341
206.124697	9629.804365	26.600359
205.940862	9652.225898	26.605376
206.295415	9653.551381	26.610394
206.826843	9679.809804	26.615412
207.095936	9688.184352	26.620429
207.477030	9700.222896	26.625447
207.433081	9712.788545	26.630464
207.755896	9718.787192	26.635482
208.046796	9744.248137	26.640500
208.064876	9754.937503	26.645517
208.513407	9760.742101	26.650535
208.306963	9779.583500	26.655552
208.660022	9792.597986	26.660570
208.863338	9812.682461	26.665588
208.658389	9824.627305	26.670605
209.437180	9842.306392	26.675623
209.212177	9857.497565	26.680640
209.336311	9871.923702	26.685658
209.694589	9894.753049	26.690676
210.054331	9920.316330	26.695693
210.481287	9918.748427	26.700711
210.376787	9936.215941	26.705728
210.452581	9946.621776	26.710746
210.718747	9964.869355	26.715764
211.250915	9975.821309	26.720781
211.600772	9983.480028	26.725799
211.950003	10011.245278	26.730816
212.416644	10006.707424	26.735834
212.327691	10012.908918	26.740852
212.331754	10031.109291	26.745869
212.458083	10040.297693	26.750887
212.881328	10058.729746	26.755904
212.947064	10079.747892	26.760922
212.800937	10087.328704	26.765940
213.019867	10106.751649	26.770957
213.499565	10113.086089	26.775975
213.435797	10128.061037	26.780992
213.871673	10148.111448	26.786010
214.159324	10156.323270	26.791028
214.154736	10183.799894	26.796045
214.402507	10194.328719	26.801063
214.218292	10206.617021	26.806080
214.725368	10221.761626	26.811098
214.924760	10239.341532	26.816116
214.834293	10257.093022	26.821133
215.270192	10275.520872	26.826151
215.326186	10299.965960	26.831168
215.807177	10316.004312	26.836186
216.346386	10325.253060	26.841204
216.181116	10354.491898	26.846221
216.123098	10363.945689	26.851239
216.333741	10385.394816	26.856256
216.773694	10400.080405	26.861274
216.833961	10429.546006	26.866292
216.893360	10452.985615	26.871309
217.522561	10466.372527	26.876327
217.833749	10492.731698	26.881344
218.291471	10488.162887	26.886362
218.645414	10509.609773	26.891380
218.487643	10521.417364	26.896397
219.390491	10532.557384	26.901415
219.547041	10544.175990	26.906432
219.613166	10549.922749	26.911450
220.056336	10548.571889	26.916468
220.157613	10572.578230	26.921485
220.606455	10581.314270	26.926503
220.337284	10581.347795	26.931520
220.954453	10594.944768	26.936538
221.309255	10608.074644	26.941556
221.023364	10619.711266	26.946573
221.356183	10615.540386	26.951591
221.384902	10642.523106	26.956608
221.442107	10660.189200	26.961626
221.429263	10671.758688	26.966644
221.403143	10688.117527	26.971661
222.274159	10708.557581	26.976679
222.663238	10725.474118	26.981696
222.744451	10751.625936	26.986714
223.053920	10752.187755	26.991732
223.043898	10765.548981	26.996749
223.597815	10775.059458	27.001767
223.305500	10794.665392	27.006784
223.799535	10814.285584	27.011802
224.085038	10824.342240	27.016820
223.913319	10847.535445	27.021837
224.393246	10856.924278	27.026855
224.248557	10886.259155	27.031872
224.447481	10897.063564	27.036890
224.874421	10919.364687	27.041908
224.962804	10951.259206	27.046925
225.427463	10956.963897	27.051943
225.761872	10983.764339	27.056960
225.877346	11003.508757	27.061978
226.008825	11016.246535	27.066996
226.378540	11034.736615	27.072013
226.910955	11042.677637	27.077031
227.168984	11061.641530	27.082048
227.242579	11065.811706	27.087066
227.479892	11077.050256	27.092084
227.567963	11095.529433	27.097101
227.829159	11110.014395	27.102119
228.062678	11127.321797	27.107136
228.258297	11158.467172	27.112154
228.786253	11150.981269	27.117172
228.747507	11166.194111	27.122189
229.107803	11186.990944	27.127207
229.533015	11193.729494	27.132224
229.305687	11195.161493	27.137242
229.707388	11203.836341	27.142260
229.746403	11228.951322	27.147277
230.028516	11243.202918	27.152295
230.371564	11256.130447	27.157312
230.444706	11256.840046	27.162330
230.741316	11284.250673	27.167348
230.854634	11301.998798	27.172365
231.125773	11313.562005	27.177383
231.379726	11324.341856	27.182400
231.219106	11343.480815	27.187418
231.721534	11370.219482	27.192436
231.597289	11401.139302	27.197453
232.003002	11404.382616	27.202471
232.322882	11424.640501	27.207488
232.681054	11449.625892	27.212506
233.314826	11456.020494	27.217524
233.216316	11482.434020	27.222541
233.668802	11496.240164	27.227559
233.577975	11516.918954	27.232576
233.858190	11551.937281	27.237594
233.824380	11556.316764	27.242612
233.722156	11564.886786	27.247629
234.266045	11594.596042	27.252647
234.552295	11627.816581	27.257664
234.587785	11640.393461	27.262682
235.140218	11663.388629	27.267700
235.619770	11697.662170	27.272717
235.940251	11707.281889	27.277735
236.426295	11714.161867	27.282752
236.301651	11740.093273	27.287770
236.745777	11749.176579	27.292788
236.862480	11770.744708	27.297805
237.152213	11787.039875	27.302823
237.488897	11795.424059	27.307840
237.796990	11809.449706	27.312858
238.176492	11817.941846	27.317876
238.426829	11830.227341	27.322893
238.445381	11832.865078	27.327911
238.997973	11843.504551	27.332928
238.800923	11854.602706	27.337946
239.133807	11875.296245	27.342964
238.769544	11892.589795	27.347981
239.351052	11921.048704	27.352999
240.025772	11948.465746	27.358016
239.909898	11952.645398	27.363034
240.297051	11970.469553	27.368052
240.195842	11999.688982	27.373069
240.553555	12012.465015	27.378087
241.103433	12029.302004	27.383104
241.215586	12050.583708	27.388122
241.574491	12063.792095	27.393140
241.643035	12077.224151	27.398157
241.976252	12084.807850	27.403175
242.260874	12101.836063	27.408192
242.125086	12119.260700	27.413210
242.507601	12139.968438	27.418228
242.580995	12164.413492	27.423245
243.161097	12172.351140	27.428263
243.358604	12203.540771	27.433280
243.381053	12214.964518	27.438298
243.899532	12232.289844	27.443316
243.819844	12251.411782	27.448333
244.333678	12265.718178	27.453351
244.725923	12286.061309	27.458368
244.756243	12300.408231	27.463386
245.603626	12293.299182	27.468404
245.832133	12308.338955	27.473421
245.868274	12324.245624	27.478439
246.221280	12332.516310	27.483456
246.251806	12340.005968	27.488474
246.487461	12354.596328	27.493492
246.283932	12368.792868	27.498509
246.366895	12375.707429	27.503527
246.776332	12401.625713	27.508544
246.818735	12428.641471	27.513562
247.275301	12440.476595	27.518580
247.243801	12468.335007	27.523597
247.491255	12495.229548	27.528615
247.860353	12512.014978	27.533632
247.881738	12540.061735	27.538650
248.398809	12558.423655	27.543668
249.032935	12582.257510	27.548685
249.237016	12610.044942	27.553703
249.347901	12602.280632	27.558720
249.920288	12643.339934	27.563738
250.171025	12642.113669	27.568756
250.341812	12655.042426	27.573773
250.336350	12678.577932	27.578791
250.895179	12685.258009	27.583808
250.760185	12705.780172	27.588826
251.212958	12723.857462	27.593844
251.539682	12754.402045	27.598861
251.582955	12770.043258	27.603879
252.256677	12778.292698	27.608896
252.222292	12814.834305	27.613914
252.459660	12824.766236	27.618932
252.657760	12844.856947	27.623949
252.590215	12865.855063	27.628967
253.297812	12883.620984	27.633984
253.369031	12912.328256	27.639002
253.428088	12930.083201	27.644020
253.934025	12960.392146	27.649037
253.866325	12963.739210	27.654055
254.667167	12988.735004	27.659072
254.648950	13031.118784	27.664090
254.965073	13032.227945	27.669108
255.319155	13062.212359	27.674125
255.416227	13082.247574	27.679143
255.616893	13097.338380	27.684160
255.996612	13125.046468	27.689178
256.339693	13139.767122	27.694196
256.444950	13173.111356	27.699213
256.647461	13185.567301	27.704231
257.022596	13201.702459	27.709248
257.086116	13215.251321	27.714266
257.359114	13230.771509	27.719284
257.719495	13263.196087	27.724301
257.638766	13277.979010	27.729319
257.922325	13301.450337	27.734336
258.021021	13339.787985	27.739354
258.272766	13362.921142	27.744372
258.798342	13391.442317	27.749389
259.320425	13420.307635	27.754407
259.906394	13436.693408	27.759424
259.724158	13464.112011	27.764442
260.122114	13477.298563	27.769460
260.334570	13496.251582	27.774477
260.287347	13529.568166	27.779495
260.746940	13548.212532	27.784512
260.810331	13567.547964	27.789530
261.140734	13591.751013	27.794548
261.260111	13602.909966	27.799565
261.717102	13613.523077	27.804583
262.397609	13639.660145	27.809600
262.557074	13663.694571	27.814618
263.109226	13659.317281	27.819636
264.124086	13672.301218	27.824653
264.411250	13685.217875	27.829671
264.559050	13681.101209	27.834688
264.590815	13676.976926	27.839706
264.716716	13681.447205	27.844724
265.180739	13706.491883	27.849741
264.721136	13708.947344	27.854759
265.283245	13717.278743	27.859776
264.680764	13733.730380	27.864794
265.099440	13759.614652	27.869812
265.533740	13773.324909	27.874829
265.591957	13806.572640	27.879847
265.928837	13837.424873	27.884864
265.945261	13865.009883	27.889882
266.370028	13877.837775	27.894900
266.626124	13903.181847	27.899917
266.600004	13937.739097	27.904935
266.915898	13953.123675	27.909952
267.196053	13991.040504	27.914970
267.291554	14005.963585	27.919988
267.861092	14037.067710	27.925005
267.545851	14084.908396	27.930023
268.154202	14096.809484	27.935040
268.871363	14139.952402	27.940058
269.449305	14165.038849	27.945076
269.679614	14178.360829	27.950093
269.937855	14204.135219	27.955111
270.411357	14225.381358	27.960128
270.545858	14251.961039	27.965146
271.170745	14254.793676	27.970164
271.323543	14279.521912	27.975181
271.257580	14294.599579	27.980199
271.796230	14304.815148	27.985216
271.860224	14330.751052	27.990234
272.244991	14354.063781	27.995252
272.511866	14374.110358	28.000269
272.138068	14402.707841	28.005287
272.162507	14414.956198	28.010304
272.851106	14450.778485	28.015322
273.412419	14480.959788	28.020340
273.725722	14496.778674	28.025357
273.748773	14525.023997	28.030375
274.217246	14547.996969	28.035392
274.753828	14571.901096	28.040410
274.897093	14588.881219	28.045428
275.043879	14607.712437	28.050445
275.182832	14632.823285	28.055463
275.552874	14654.665428	28.060480
276.212832	14677.211400	28.065498
276.093937	14702.059232	28.070516
276.923467	14721.445959	28.075533
276.375993	14743.922033	28.080551
276.600511	14764.595416	28.085568
277.055831	14796.170573	28.090586
277.227229	14823.230467	28.095604
277.763719	14852.557696	28.100621
277.646324	14878.325877	28.105639
278.369889	14903.526512	28.110656
278.578133	14932.731615	28.115674
278.585478	14945.490639	28.120692
278.964826	14967.296994	28.125709
278.995746	15008.855186	28.130727
279.652175	15022.876505	28.135744
279.998093	15047.747352	28.140762
280.088641	15085.360810	28.145780
280.529124	15093.757143	28.150797
280.796909	15112.605200	28.155815
280.859051	15139.437825	28.160832
281.216593	15166.185443	28.165850
281.348155	15185.415403	28.170868
282.172208	15208.190303	28.175885
282.069457	15240.192622	28.180903
282.722578	15248.066939	28.185920
282.972807	15274.994787	28.190938
283.012427	15291.075566	28.195956
283.842605	15306.817725	28.200973
283.757426	15325.771622	28.205991
283.922833	15352.176213	28.211008
284.394608	15380.733414	28.216026
284.309862	15401.105686	28.221044
284.994983	15413.530887	28.226061
284.808404	15441.263997	28.231079
285.259540	15445.357957	28.236096
285.797691	15479.877258	28.241114
285.781278	15497.808224	28.246132
286.322456	15524.390558	28.251149
286.632986	15546.045158	28.256167
287.203665	15560.353752	28.261184
287.936549	15574.214775	28.266202
287.803895	15585.560141	28.271220
288.306557	15613.173366	28.276237
288.452469	15617.377685	28.281255
288.315617	15639.875401	28.286272
288.507070	15673.300349	28.291290
288.596100	15692.619885	28.296308
289.271566	15711.714901	28.301325
289.523728	15740.841700	28.306343
289.670484	15762.295126	28.311360
290.059908	15784.208078	28.316378
290.420561	15816.016763	28.321396
291.077697	15821.849782	28.326413
291.251127	15848.569049	28.331431
291.091339	15885.212340	28.336448
291.770259	15894.776913	28.341466
291.872787	15912.813188	28.346484
292.089621	15937.656287	28.351501
292.258544	15967.054130	28.356519
292.748904	15989.369901	28.361536
293.000190	16006.417182	28.366554
292.907820	16038.175063	28.371572
293.669432	16057.101803	28.376589
294.019795	16082.153160	28.381607
294.675936	16103.890090	28.386624
295.102438	16125.863568	28.391642
295.207583	16142.493849	28.396660
295.360272	16151.612817	28.401677
295.636837	16177.480287	28.406695
295.644214	16202.810715	28.411712
296.188745	16213.980018	28.416730
296.454676	16255.482062	28.421748
296.732044	16265.442589	28.426765
296.383704	16294.199923	28.431783
296.737652	16323.890926	28.436800
297.217674	16352.308197	28.441818
297.330519	16379.474904	28.446836
297.738999	16404.008088	28.451853
297.997169	16443.697853	28.456871
298.156853	16467.299809	28.461888
298.597167	16492.797142	28.466906
298.964070	16534.971950	28.471924
299.058758	16544.449031	28.476941
299.105089	16583.751748	28.481959
299.950691	16606.915911	28.486976
300.415313	16624.820648	28.491994
300.108076	16654.060403	28.497012
300.641559	16676.882213	28.502029
301.294447	16710.935975	28.507047
301.317503	16725.288785	28.512064
301.537104	16746.919019	28.517082
301.321592	16787.956624	28.522100
301.964667	16818.675649	28.527117
302.134495	16840.968309	28.532135
302.458398	16881.221971	28.537152
303.182731	16902.874622	28.542170
303.017393	16929.222919	28.547188
303.103725	16960.948331	28.552205
303.673303	16999.215202	28.557223
304.097518	17029.802138	28.562240
304.607618	17060.121187	28.567258
304.803778	17085.807934	28.572276
305.515230	17114.692649	28.577293
305.680122	17139.519355	28.582311
305.823655	17168.756476	28.587328
306.454968	17194.803361	28.592346
306.387913	17233.718145	28.597364
306.921855	17237.188919	28.602381
307.323473	17269.761233	28.607399
307.869122	17312.201667	28.612416
308.129830	17317.404069	28.617434
308.212702	17340.480929	28.622452
308.874029	17363.394480	28.627469
309.284811	17372.506163	28.632487
309.341159	17420.597814	28.637504
310.183674	17436.221786	28.642522
310.457491	17449.201951	28.647540
310.681224	17459.640183	28.652557
311.166174	17504.934525	28.657575
311.099775	17502.281867	28.662592
311.508946	17512.564980	28.667610
311.365884	17544.925204	28.672628
311.832297	17561.922799	28.677645
312.224169	17587.398314	28.682663
312.528287	17621.721216	28.687680
312.831908	17629.164245	28.692698
312.786911	17670.119133	28.697716
313.362021	17689.992759	28.702733
313.864864	17708.828614	28.707751
314.093027	17734.444887	28.712768
314.566559	17744.982311	28.717786
314.569299	17773.187724	28.722804
314.909196	17792.443065	28.727821
315.517466	17831.093223	28.732839
315.957389	17842.082324	28.737856
316.026734	17864.416614	28.742874
316.298329	17897.870678	28.747892
316.637422	17914.036951	28.752909
316.888020	17938.253323	28.757927
316.973148	17970.858822	28.762944
317.471126	17986.860211	28.767962
317.464505	18018.068681	28.772980
317.906055	18047.844475	28.777997
318.600867	18073.276998	28.783015
318.732877	18104.976575	28.788032
319.051531	18131.992381	28.793050
319.135687	18164.634675	28.798068
319.210894	18181.602969	28.803085
319.358858	18214.690349	28.808103
319.639137	18256.719952	28.813120
320.221314	18284.294591	28.818138
320.386378	18321.985112	28.823156
320.525976	18350.975933	28.828173
320.817039	18378.907767	28.833191
321.162590	18406.548498	28.838208
321.608488	18433.428709	28.843226
321.878587	18487.854615	28.848244
322.398315	18500.317377	28.853261
322.843397	18540.099534	28.858279
323.211028	18574.070299	28.863296
323.506654	18587.747618	28.868314
323.470560	18630.544484	28.873332
323.967942	18665.851167	28.878349
324.396170	18692.517194	28.883367
324.682860	18731.558334	28.888384
325.402113	18756.905907	28.893402
325.072639	18792.773482	28.898420
325.367402	18825.654982	28.903437
326.167908	18855.374505	28.908455
326.050581	18898.726151	28.913472
326.527242	18926.141172	28.918490
326.896014	18949.611255	28.923508
327.106237	18982.469201	28.928525
327.263179	19036.631869	28.933543
327.601267	19065.378347	28.938560
328.118825	19089.624812	28.943578
328.563607	19138.992418	28.948596
328.775652	19175.803842	28.953613
329.184458	19204.600354	28.958631
329.286798	19244.847517	28.963648
330.010011	19291.702632	28.968666
330.227664	19324.973027	28.973684
330.730293	19343.575912	28.978701
331.393307	19374.138776	28.983719
331.742841	19409.041128	28.988736
331.839142	19438.151347	28.993754
332.353955	19463.062452	28.998772
332.809285	19488.639182	29.003789
333.616794	19519.148491	29.008807
333.540387	19530.846679	29.013824
333.871002	19550.488656	29.018842
334.301248	19587.398933	29.023860
334.493899	19602.806027	29.028877
334.792186	19643.954988	29.033895
334.983700	19673.705655	29.038912
335.578059	19690.736328	29.043930
336.085705	19731.797323	29.048948
335.717289	19758.740126	29.053965
336.047652	19776.375689	29.058983
336.209107	19803.585711	29.064000
336.941236	19832.027232	29.069018
337.243128	19872.674875	29.074036
337.511993	19912.240367	29.079053
338.022726	19930.420100	29.084071
338.115952	19961.800166	29.089088
338.289117	19992.039962	29.094106
338.670239	20037.738299	29.099124
338.814469	20071.241436	29.104141
339.134968	20111.498793	29.109159
339.382144	20144.791173	29.114176
339.669584	20176.667654	29.119194
340.101320	20218.853762	29.124212
340.339239	20256.109427	29.129229
341.116029	20288.646197	29.134247
341.426768	20334.593439	29.139264
341.669444	20372.152828	29.144282
341.970653	20411.134033	29.149300
342.434632	20452.405803	29.154317
343.218676	20487.706837	29.159335
343.360814	20506.811985	29.164352
343.735801	20543.452905	29.169370
343.833250	20556.617561	29.174388
344.287957	20582.389980	29.179405
345.053410	20613.441089	29.184423
345.065293	20637.705568	29.189440
345.386362	20662.741914	29.194458
345.659302	20690.882416	29.199476
346.074226	20717.027354	29.204493
346.584104	20739.261201	29.209511
346.713845	20776.356182	29.214528
347.029096	20795.513462	29.219546
347.644513	20829.914538	29.224564
348.223192	20865.981785	29.229581
348.402117	20886.233695	29.234599
348.705569	20915.925521	29.239616
349.024353	20946.191860	29.244634
349.234758	20969.076128	29.249652
349.498849	21001.848759	29.254669
350.264165	21030.428733	29.259687
350.628889	21054.044340	29.264704
350.792895	21077.893355	29.269722
350.933488	21110.853711	29.274740
351.259130	21151.826881	29.279757
351.799728	21181.223031	29.284775
351.810228	21228.196612	29.289792
352.145284	21253.310358	29.294810
352.793329	21287.836262	29.299828
352.863679	21328.807898	29.304845
353.137035	21352.984498	29.309863
352.887429	21394.141579	29.314880
353.678150	21435.063834	29.319898
354.150626	21469.745241	29.324916
354.512596	21513.525831	29.329933
355.021442	21558.135181	29.334951
355.280809	21596.162794	29.339968
355.429094	21636.170072	29.344986
355.820919	21676.261759	29.350004
356.026933	21724.347430	29.355021
356.512278	21753.763173	29.360039
356.988384	21797.818890	29.365056
357.625679	21835.880782	29.370074
358.044577	21869.793043	29.375092
358.464888	21903.963698	29.380109
359.097091	21927.380268	29.385127
359.484537	21961.178090	29.390144
359.374023	21988.587949	29.395162
360.087426	22014.726597	29.400180
360.089929	22059.439848	29.405197
360.654474	22089.669230	29.410215
361.069073	22124.035197	29.415232
361.692419	22164.722018	29.420250
361.926970	22182.845780	29.425268
362.122975	22212.715314	29.430285
362.640539	22255.338557	29.435303
363.241670	22276.805756	29.440320
363.358685	22305.403568	29.445338
363.920152	22333.283168	29.450356
364.099981	22376.960511	29.455373
364.245851	22399.229899	29.460391
364.669662	22435.313498	29.465408
364.884196	22476.581014	29.470426
365.435542	22497.433952	29.475444
365.661610	22537.367459	29.480461
365.839711	22567.688345	29.485479
366.076502	22602.240751	29.490496
366.913878	22643.678541	29.495514
367.615671	22662.852932	29.500532
367.876524	22688.595977	29.505549
368.496196	22710.281399	29.510567
368.880165	22743.472782	29.515584
369.019253	22759.246379	29.520602
369.048209	22792.163832	29.525620
369.321803	22809.630660	29.530637
369.945728	22841.660014	29.535655
369.874539	22871.314708	29.540672
370.117298	22896.835598	29.545690
370.717648	22931.672333	29.550708
370.804452	22983.842800	29.555725
371.466902	23019.028939	29.560743
371.914389	23051.707475	29.565760
372.083404	23084.460459	29.570778
372.925572	23120.922617	29.575796
373.102266	23155.465588	29.580813
373.504873	23186.321260	29.585831
373.509971	23217.677827	29.590848
373.740209	23249.393009	29.595866
374.154787	23293.273603	29.600884
374.223532	23344.205723	29.605901
374.561030	23376.879409	29.610919
374.891710	23431.390228	29.615936
375.239389	23480.119727	29.620954
376.012554	23526.078145	29.625972
376.433885	23562.773184	29.630989
377.046869	23596.560680	29.636007
377.270476	23647.121247	29.641024
377.337358	23698.483613	29.646042
377.918545	23724.523779	29.651060
378.145516	23774.943842	29.656077
378.439410	23812.494575	29.661095
378.858848	23857.498478	29.666112
379.369662	23899.728073	29.671130
380.075678	23947.582960	29.676148
379.972659	23986.948282	29.681165
380.512414	24031.835012	29.686183
381.109768	24073.350657	29.691200
381.440323	24119.123638	29.696218
381.816950	24153.739685	29.701236
382.534722	24203.614791	29.706253
383.030175	24227.266868	29.711271
383.547607	24263.804063	29.716288
383.969863	24299.287990	29.721306
384.634444	24330.052015	29.726324
384.470614	24376.695763	29.731341
384.855099	24401.175316	29.736359
385.167500	24443.784366	29.741376
385.522867	24490.650134	29.746394
385.924857	24515.776609	29.751412
385.959635	24568.964984	29.756429
386.434265	24602.291683	29.761447
387.079809	24643.058078	29.766464
387.212574	24693.048611	29.771482
387.661106	24733.321105	29.776500
387.823552	24779.251361	29.781517
388.052438	24816.086553	29.786535
388.433636	24860.262127	29.791552
388.697516	24910.876571	29.796570
389.324926	24955.642462	29.801588
389.526615	25007.798598	29.806605
390.058451	25055.945569	29.811623
390.675752	25092.703002	29.816640
390.745001	25155.992110	29.821658
391.419816	25195.425687	29.826676
391.840222	25245.252057	29.831693
392.094529	25283.372375	29.836711
392.724410	25335.122899	29.841728
392.835360	25367.833114	29.846746
393.450564	25414.336814	29.851764
393.842614	25450.879928	29.856781
394.056217	25494.744223	29.861799
394.699209	25527.280122	29.866816
395.012601	25571.774664	29.871834
395.712229	25594.896613	29.876852
396.085178	25635.137996	29.881869
396.083406	25678.667767	29.886887
396.829462	25713.755808	29.891904
396.888750	25756.506148	29.896922
397.541034	25791.281838	29.901940
397.768813	25838.926168	29.906957
398.584321	25876.035746	29.911975
398.857788	25911.355228	29.916992
398.922460	25953.458623	29.922010
399.225992	25991.331117	29.927028
400.061869	26035.947137	29.932045
400.260203	26074.032736	29.937063
400.912527	26109.728438	29.942080
401.197226	26156.643577	29.947098
401.696161	26193.169046	29.952116
402.560378	26216.602123	29.957133
403.071419	26257.967046	29.962151
403.472432	26283.523653	29.967168
403.784457	26311.258621	29.972186
404.057759	26339.170345	29.977204
404.479481	26387.214681	29.982221
404.833005	26429.271530	29.987239
405.048370	26449.711743	29.992256
405.253577	26487.942211	29.997274
405.458448	26538.669002	30.002292
406.246137	26576.752981	30.007309
406.217891	26619.961499	30.012327
406.776625	26671.393499	30.017344
407.174423	26713.503658	30.022362
408.257777	26737.077877	30.027380
408.761851	26775.761109	30.032397
408.889664	26814.588591	30.037415
409.399768	26840.462339	30.042432
409.665262	26890.448412	30.047450
410.035971	26930.459811	30.052468
410.162144	26960.743489	30.057485
410.065418	27014.047930	30.062503
410.510773	27054.920972	30.067520
410.842023	27120.197417	30.072538
411.426945	27180.085958	30.077556
412.132550	27223.351397	30.082573
412.242958	27276.086228	30.087591
412.760955	27324.382233	30.092608
412.876010	27369.278513	30.097626
413.366281	27418.989274	30.102644
413.778382	27473.658847	30.107661
414.054536	27518.853784	30.112679
414.715198	27565.019899	30.117696
415.126883	27621.443744	30.122714
415.449642	27674.668315	30.127732
415.724664	27712.312752	30.132749
415.965688	27773.979223	30.137767
416.607089	27826.003482	30.142784
417.174418	27885.569343	30.147802
417.813090	27939.979016	30.152820
418.546142	27965.357107	30.157837
418.554221	28008.831222	30.162855
419.468008	28061.672316	30.167872
419.940116	28100.732862	30.172890
420.689875	28127.505786	30.177908
420.920586	28163.890500	30.182925
421.606062	28211.823817	30.187943
422.258395	28216.151105	30.192960
422.135087	28261.451829	30.197978
422.621028	28294.271275	30.202996
423.154633	28312.418404	30.208013
423.113163	28356.800565	30.213031
423.917997	28396.854060	30.218048
424.078732	28427.699235	30.223066
424.374332	28469.515138	30.228084
425.052193	28509.987320	30.233101
424.945795	28545.009058	30.238119
425.361127	28587.319630	30.243136
426.040251	28630.520429	30.248154
426.124570	28677.087552	30.253172
426.521092	28721.048156	30.258189
426.750751	28775.026476	30.263207
427.336061	28813.798655	30.268224
427.529419	28862.357633	30.273242
427.992920	28913.376749	30.278260
428.638501	28969.375210	30.283277
428.727992	29031.926057	30.288295
429.231495	29081.806608	30.293312
429.833782	29144.263687	30.298330
430.070480	29181.829330	30.303348
430.766280	29240.558471	30.308365
431.027132	29307.867387	30.313383
432.120161	29337.329914	30.318400
432.148336	29387.605317	30.323418
432.632379	29440.452219	30.328436
433.412918	29481.423903	30.333453
434.120350	29516.956692	30.338471
434.606458	29563.806824	30.343488
435.330702	29599.769181	30.348506
435.469589	29634.963954	30.353524
436.312524	29672.534616	30.358541
436.163310	29707.518452	30.363559
437.135483	29752.459139	30.368576
437.165305	29799.123449	30.373594
437.843880	29838.598611	30.378612
437.938633	29873.684437	30.383629
437.816484	29919.932527	30.388647
438.397991	29980.197272	30.393664
439.459226	30030.732914	30.398682
439.034547	30062.494753	30.403700
440.018238	30115.428368	30.408717
440.364296	30167.325483	30.413735
440.497990	30210.554072	30.418752
440.612177	30267.833817	30.423770
441.247559	30327.374749	30.428788
442.226961	30364.287116	30.433805
442.297160	30421.555704	30.438823
442.783136	30463.688825	30.443840
443.381604	30524.022054	30.448858
444.071912	30566.702143	30.453876
444.555668	30604.854687	30.458893
444.943231	30662.462828	30.463911
445.540144	30705.180767	30.468928
445.789197	30737.495040	30.473946
446.327168	30793.586560	30.478964
447.127157	30834.447805	30.483981
447.274910	30875.249683	30.488999
447.456355	30923.355778	30.494016
448.167269	30965.377239	30.499034
448.436293	31009.323678	30.504052
449.100394	31058.173824	30.509069
449.242693	31103.725159	30.514087
449.752558	31145.988485	30.519104
450.214369	31193.436969	30.524122
450.253938	31239.087652	30.529140
451.457102	31279.656190	30.534157
451.362051	31324.322928	30.539175
451.465473	31364.994456	30.544192
452.041749	31411.840971	30.549210
452.430072	31448.982627	30.554228
452.978503	31512.924126	30.559245
453.387141	31557.337889	30.564263
453.887595	31612.920827	30.569280
454.230817	31669.643609	30.574298
454.506493	31717.916152	30.579316
454.921715	31774.744113	30.584333
455.557849	31843.149219	30.589351
455.884213	31882.094053	30.594368
456.807511	31932.525483	30.599386
457.266952	31994.148745	30.604404
458.120587	32028.794882	30.609421
458.323177	32091.249664	30.614439
458.885810	32126.669718	30.619456
459.380486	32161.457443	30.624474
459.928315	32210.200654	30.629492
460.649887	32248.790755	30.634509
460.860391	32297.340680	30.639527
461.444358	32334.985100	30.644544
462.034505	32377.339096	30.649562
462.100709	32424.849952	30.654580
462.650307	32469.009261	30.659597
462.815650	32524.274985	30.664615
463.340426	32563.838505	30.669632
463.837505	32622.826398	30.674650
464.064335	32677.505060	30.679668
464.417884	32730.607479	30.684685
464.487163	32789.770716	30.689703
464.912041	32854.554688	30.694720
465.470247	32911.747633	30.699738
465.889535	32965.499330	30.704756
466.483643	33031.776793	30.709773
467.110805	33108.092042	30.714791
467.640755	33158.225963	30.719808
468.012544	33218.400816	30.724826
468.164916	33280.539964	30.729844
468.680986	33334.920465	30.734861
469.072730	33389.807579	30.739879
469.827411	33471.192751	30.744896
470.573571	33531.117512	30.749914
470.738916	33592.630869	30.754932
471.365460	33656.160218	30.759949
471.759487	33714.474615	30.764967
472.443437	33775.934496	30.769984
472.738192	33831.167153	30.775002
472.869886	33894.744391	30.780020
473.591062	33958.489533	30.785037
474.243892	34026.660547	30.790055
474.476929	34088.429493	30.795072
475.222149	34153.171617	30.800090
475.481446	34210.172017	30.805108
476.340768	34276.486064	30.810125
476.259280	34327.610968	30.815143
476.958657	34395.147782	30.820160
477.591212	34450.408609	30.825178
477.871503	34506.466172	30.830196
478.610198	34567.528479	30.835213
479.195935	34635.053422	30.840231
479.818682	34688.398084	30.845248
480.527219	34743.521054	30.850266
480.705964	34800.419900	30.855284
481.227888	34851.913651	30.860301
481.818488	34896.094338	30.865319
482.303749	34953.094506	30.870336
483.001631	34991.596695	30.875354
483.255993	35057.855812	30.880372
483.904430	35091.970711	30.885389
484.316550	35134.594230	30.890407
484.847403	35195.282803	30.895424
485.069632	35241.314405	30.900442
485.376193	35288.294649	30.905460
485.902271	35346.949174	30.910477
485.819939	35405.423541	30.915495
486.862440	35463.563983	30.920512
487.205780	35523.423163	30.925530
487.482671	35595.695185	30.930548
487.998288	35633.433648	30.935565
488.407542	35695.608229	30.940583
488.878241	35767.508121	30.945600
489.363158	35823.463445	30.950618
489.904295	35887.147414	30.955636
490.733580	35952.081008	30.960653
490.930375	36012.196398	30.965671
491.670266	36061.306631	30.970688
492.650677	36122.271226	30.975706
493.019411	36173.099835	30.980724
493.789426	36211.924099	30.985741
494.231207	36271.693786	30.990759
494.110752	36344.750825	30.995776
494.948428	36399.403152	31.000794
495.503565	36462.695540	31.005812
495.861022	36514.628352	31.010829
495.990845	36574.362215	31.015847
496.542778	36631.318856	31.020864
497.328756	36688.681990	31.025882
497.727021	36768.345438	31.030900
498.297304	36820.057785	31.035917
498.724497	36878.124585	31.040935
499.209620	36944.690249	31.045952
499.806134	37008.321718	31.050970
500.159970	37059.521383	31.055988
500.797313	37123.664084	31.061005
501.466635	37175.660907	31.066023
502.343290	37236.242476	31.071040
503.023618	37285.965532	31.076058
503.082242	37346.439587	31.081076
503.686727	37395.616870	31.086093
503.972416	37464.524407	31.091111
504.386597	37524.419593	31.096128
504.775990	37579.493563	31.101146
505.207651	37647.929539	31.106164
506.069191	37701.859166	31.111181
506.555707	37772.748243	31.116199
506.583894	37836.321871	31.121216
507.375147	37889.127497	31.126234
508.435505	37941.860423	31.131252
508.957154	38000.950428	31.136269
509.680759	38044.321588	31.141287
509.870449	38108.207196	31.146304
510.888537	38149.522699	31.151322
510.850904	38206.152481	31.156340
511.155211	38267.984037	31.161357
511.850686	38326.162683	31.166375
512.109543	38390.489187	31.171392
512.750005	38440.865866	31.176410
512.817256	38510.507826	31.181428
513.304623	38567.026768	31.186445
514.014416	38626.558009	31.191463
513.989621	38704.999549	31.196480
514.725261	38752.561839	31.201498
515.407224	38823.561626	31.206516
515.975856	38886.831895	31.211533
516.457789	38938.325040	31.216551
516.515480	39004.063065	31.221568
517.036484	39063.374427	31.226586
517.468240	39128.363053	31.231604
517.754273	39198.072514	31.236621
518.421373	39273.059732	31.241639
518.670394	39341.431278	31.246656
519.302705	39405.800699	31.251674
520.057077	39483.877023	31.256692
520.351391	39555.761193	31.261709
520.605767	39627.062006	31.266727
521.197627	39712.106959	31.271744
522.227851	39771.775257	31.276762
523.196999	39844.019398	31.281780
524.002878	39899.426178	31.286797
524.645769	39966.030562	31.291815
524.870067	40021.338079	31.296832
526.108414	40051.845551	31.301850
527.295623	40105.305590	31.306868
527.790843	40138.161237	31.311885
528.659700	40187.270876	31.316903
529.093850	40237.648745	31.321920
529.637976	40267.109675	31.326938
529.882016	40315.707355	31.331956
530.482654	40376.471290	31.336973
530.906795	40401.874090	31.341991
530.866381	40463.517538	31.347008
531.437886	40513.406320	31.352026
531.780131	40576.363177	31.357044
532.124744	40622.618713	31.362061
532.416967	40676.114623	31.367079
532.686073	40751.842853	31.372096
533.239699	40803.878673	31.377114
533.816622	40875.001669	31.382132
534.038263	40942.354701	31.387149
534.780705	41014.303173	31.392167
534.924813	41096.922208	31.397184
535.592095	41169.028907	31.402202
535.983453	41233.886506	31.407220
536.613164	41315.100534	31.412237
537.362513	41385.881369	31.417255
537.937662	41455.239187	31.422272
538.260792	41531.507817	31.427290
539.043445	41616.782656	31.432308
539.332018	41683.189815	31.437325
539.629515	41760.710527	31.442343
540.207519	41845.590917	31.447360
540.994015	41918.021795	31.452378
541.475191	41998.136421	31.457396
541.920149	42070.744270	31.462413
543.237386	42141.885639	31.467431
543.612126	42217.236279	31.472448
543.853270	42291.213985	31.477466
544.623535	42364.912027	31.482484
545.144561	42431.854876	31.487501
545.727094	42495.668852	31.492519
546.434597	42580.332359	31.497536
546.908756	42641.512982	31.502554
547.493501	42695.427358	31.507572
547.838863	42779.794870	31.512589
548.410305	42844.432675	31.517607
548.225251	42930.706859	31.522624
548.874222	43018.011751	31.527642
549.526401	43083.663059	31.532660
549.837114	43171.106625	31.537677
550.615884	43244.601573	31.542695
551.049713	43326.595554	31.547712
551.366661	43399.959038	31.552730
552.047614	43475.939831	31.557748
552.693020	43548.675076	31.562765
553.350033	43617.424517	31.567783
553.943279	43709.209073	31.572800
554.414171	43774.416060	31.577818
555.132783	43848.229575	31.582836
555.527410	43937.809705	31.587853
556.209842	43997.021958	31.592871
556.861915	44078.879034	31.597888
557.081350	44160.350147	31.602906
558.019259	44230.507740	31.607924
558.173632	44317.613147	31.612941
558.945235	44398.994103	31.617959
559.840804	44467.249500	31.622976
560.206418	44525.458112	31.627994
560.906233	44612.275904	31.633012
560.975576	44681.678859	31.638029
561.669899	44761.947042	31.643047
562.399662	44846.595123	31.648064
563.038940	44907.724377	31.653082
563.815832	44992.327448	31.658100
564.249850	45070.256219	31.663117
565.190166	45143.233148	31.668135
565.038380	45222.916890	31.673152
565.731248	45310.215830	31.678170
566.767280	45378.650278	31.683188
566.766345	45466.708640	31.688205
567.831553	45549.823710	31.693223
568.264685	45633.113011	31.698240
568.459111	45708.829653	31.703258
569.226061	45804.858310	31.708276
569.692471	45882.210467	31.713293
570.553076	45963.220441	31.718311
571.394878	46054.328215	31.723328
571.642296	46121.755799	31.728346
572.470548	46199.324197	31.733364
573.188432	46281.732620	31.738381
573.804605	46353.940551	31.743399
574.359196	46427.781890	31.748416
574.784948	46519.563724	31.753434
575.699098	46577.246068	31.758452
575.890386	46659.973626	31.763469
576.783509	46740.245877	31.768487
577.244865	46817.132243	31.773504
578.057847	46879.164412	31.778522
578.868605	46957.212467	31.783540
579.149003	47031.489848	31.788557
579.869757	47108.157733	31.793575
580.153411	47186.306428	31.798592
580.791506	47249.341253	31.803610
581.237581	47327.160572	31.808628
582.005104	47410.421465	31.813645
582.787078	47470.673463	31.818663
583.594371	47547.609875	31.823680
583.634352	47626.324814	31.828698
584.616087	47686.326626	31.833716
584.830233	47770.122584	31.838733
585.006485	47846.052916	31.843751
585.970894	47918.398792	31.848768
586.531448	48006.155246	31.853786
587.080817	48082.381728	31.858804
587.665006	48166.655145	31.863821
588.498925	48230.169306	31.868839
588.838597	48320.114163	31.873856
588.947334	48402.982983	31.878874
589.734562	48475.009731	31.883892
590.271031	48553.037051	31.888909
591.210091	48630.240309	31.893927
591.755905	48701.158323	31.898944
592.344099	48789.791730	31.903962
593.331935	48849.275169	31.908980
593.477312	48924.160172	31.913997
594.084033	48984.733307	31.919015
594.299110	49054.181983	31.924032
594.489486	49141.534292	31.929050
595.933130	49212.403821	31.934068
596.341089	49284.679443	31.939085
596.886085	49376.067003	31.944103
597.322633	49461.355844	31.949120
597.485768	49547.264984	31.954138
598.354492	49640.536213	31.959156
598.804612	49713.747594	31.964173
599.442983	49774.725403	31.969191
600.170348	49877.849035	31.974208
600.460207	49972.101754	31.979226
601.890762	50045.446178	31.984244
603.224019	50115.970963	31.989261
604.008842	50185.670732	31.994279
604.902778	50255.520116	31.999296
604.960210	50317.732540	32.004314
606.077319	50377.660493	32.009332
606.456281	50442.545713	32.014349
607.042962	50521.078103	32.019367
607.602041	50576.465787	32.024384
607.587752	50656.936062	32.029402
608.354659	50738.613577	32.034420
608.743888	50831.319216	32.039437
609.068321	50895.779138	32.044455
609.946148	50978.718446	32.049472
610.087097	51061.782976	32.054490
610.796252	51146.007858	32.059508
611.528483	51235.121511	32.064525
612.196692	51317.383126	32.069543
612.571298	51401.534892	32.074560
613.205664	51489.952106	32.079578
613.941681	51575.428296	32.084596
614.748624	51664.348412	32.089613
615.441421	51740.584756	32.094631
616.147426	51835.381141	32.099648
616.127489	51911.448461	32.104666
616.885627	52002.478544	32.109684
617.396173	52100.249009	32.114701
617.960492	52194.647328	32.119719
618.946238	52268.907556	32.124736
619.340791	52375.036940	32.129754
620.119864	52441.893725	32.134772
620.832539	52535.261642	32.139789
621.242156	52640.019194	32.144807
622.192757	52714.429074	32.149824
622.628780	52810.231869	32.154842
623.014535	52908.582936	32.159860
623.430024	53007.656066	32.164877
624.103801	53090.685535	32.169895
624.397686	53193.961696	32.174912
625.067397	53293.082736	32.179930
625.505053	53388.186895	32.184948
626.220828	53479.777365	32.189965
626.902724	53594.697605	32.194983
627.372851	53700.310045	32.200000
628.433794	53789.886570	32.205018
629.244990	53889.448456	32.210036
629.819381	53992.663573	32.215053
630.234760	54078.810245	32.220071
631.007040	54179.251858	32.225088
631.748103	54283.944570	32.230106
632.349225	54362.998744	32.235124
633.465379	54452.202774	32.240141
633.819855	54531.089880	32.245159
634.928815	54594.557537	32.250176
635.239295	54686.972423	32.255194
636.063287	54758.719683	32.260212
636.711230	54850.087718	32.265229
637.249993	54921.219314	32.270247
638.034446	55001.351407	32.275264
638.666872	55082.311304	32.280282
639.246248	55160.904773	32.285300
639.768580	55260.306543	32.290317
640.434084	55334.855655	32.295335
640.970537	55412.869654	32.300352
641.494870	55516.132666	32.305370
642.394988	55606.559104	32.310388
642.532345	55684.242058	32.315405
642.914460	55778.267674	32.320423
644.161747	55878.904913	32.325440
644.554885	55969.682112	32.330458
645.289684	56057.718080	32.335476
646.147933	56150.472703	32.340493
646.774674	56239.298149	32.345511
647.440688	56321.925618	32.350528
647.987185	56425.897386	32.355546
648.863045	56506.557575	32.360564
649.377395	56599.219466	32.365581
649.720738	56710.561883	32.370599
650.511056	56790.390697	32.375616
651.268819	56882.255506	32.380634
651.807433	56986.187294	32.385652
652.812741	57081.082919	32.390669
653.478938	57169.716478	32.395687
654.099743	57262.780919	32.400704
654.348464	57356.956133	32.405722
655.217062	57444.672892	32.410740
655.989342	57548.354205	32.415757
656.511269	57637.418075	32.420775
657.330164	57737.231966	32.425792
657.892153	57833.316502	32.430810
658.535506	57931.624908	32.435828
659.264100	58008.517958	32.440845
659.745785	58118.872338	32.445863
660.581002	58212.392367	32.450880
661.014684	58322.010175	32.455898
661.730686	58412.397706	32.460916
662.198369	58515.325543	32.465933
662.292682	58635.850769	32.470951
663.544915	58726.353371	32.475968
664.150885	58827.553844	32.480986
664.944570	58941.456788	32.486004
665.584468	59034.001873	32.491021
666.138462	59142.567980	32.496039
667.016908	59238.840832	32.501056
667.434235	59343.013488	32.506074
668.616564	59449.847133	32.511092
669.169442	59544.753393	32.516109
669.333012	59651.604701	32.521127
670.611169	59738.777329	32.526144
670.950061	59850.384480	32.531162
671.658738	59945.538639	32.536180
672.730545	60040.096125	32.541197
673.738786	60135.081639	32.546215
675.093119	60204.226926	32.551232
675.759715	60302.814889	32.556250
676.304282	60374.173616	32.561268
677.215761	60448.183093	32.566285
677.699015	60539.124225	32.571303
678.437866	60611.342770	32.576320
678.793925	60683.681668	32.581338
679.353416	60761.422137	32.586356
680.228529	60846.852395	32.591373
680.346743	60921.266365	32.596391
680.663485	61001.790603	32.601408
681.693556	61096.119794	32.606426
681.951822	61193.363919	32.611444
682.581879	61271.473885	32.616461
682.861860	61373.922823	32.621479
683.853628	61471.875049	32.626496
684.077249	61573.588559	32.631514
684.247650	61678.768379	32.636532
685.185966	61790.799181	32.641549
685.414395	61902.202078	32.646567
686.317430	62018.227894	32.651584
687.303561	62123.155217	32.656602
687.773653	62235.531245	32.661620
688.623629	62362.324636	32.666637
689.260044	62471.672425	32.671655
690.500444	62584.441420	32.676672
690.911806	62704.003194	32.681690
691.172544	62815.462637	32.686708
692.096667	62918.324924	32.691725
692.143761	63050.880290	32.696743
693.545260	63161.527511	32.701760
694.308987	63271.427399	32.706778
694.627538	63404.660759	32.711796
695.755301	63507.549268	32.716813
696.431806	63623.931342	32.721831
697.372197	63749.429028	32.726848
698.085481	63853.007143	32.731866
698.954569	63963.904649	32.736884
699.959388	64068.023526	32.741901
700.737974	64182.040615	32.746919
701.342447	64283.344451	32.751936
702.022459	64393.972111	32.756954
702.573278	64502.441019	32.761972
703.623421	64603.736042	32.766989
704.083274	64711.854467	32.772007
705.156545	64834.005732	32.777024
705.548761	64926.441611	32.782042
706.057399	65037.834263	32.787060
706.988227	65148.449839	32.792077
707.613414	65260.842131	32.797095
708.669694	65363.138601	32.802112
709.492584	65477.193471	32.807130
710.161582	65580.066984	32.812148
710.952637	65679.437881	32.817165
711.090444	65789.707444	32.822183
712.305849	65891.139527	32.827200
712.735370	66006.829948	32.832218
713.180036	66130.319017	32.837236
713.776984	66223.567617	32.842253
714.394655	66347.231688	32.847271
714.951886	66462.713917	32.852288
715.843585	66587.383519	32.857306
716.337161	66710.924853	32.862324
717.217696	66823.858705	32.867341
717.487005	66959.247167	32.872359
718.298838	67067.231253	32.877376
719.729286	67178.419953	32.882394
720.002248	67302.677643	32.887412
721.166003	67408.171534	32.892429
721.633430	67542.216144	32.897447
722.284772	67662.639405	32.902464
722.938994	67780.945075	32.907482
723.428922	67900.606134	32.912500
724.748352	67996.872672	32.917517
725.206971	68114.175738	32.922535
726.105916	68218.832382	32.927552
727.378443	68306.927490	32.932570
728.570022	68397.893883	32.937588
729.650962	68480.186151	32.942605
730.295549	68579.348504	32.947623
730.655681	68667.975129	32.952640
731.780971	68756.121728	32.957658
732.388919	68848.994583	32.962676
733.276018	68946.519118	32.967693
733.734281	69030.452660	32.972711
734.235412	69134.635854	32.977728
735.098390	69239.417323	32.982746
735.059698	69340.251373	32.987764
735.538080	69435.190305	32.992781
735.714176	69561.645909	32.997799
736.481966	69671.970980	33.002816
737.087265	69794.032584	33.007834
737.845449	69922.126559	33.012852
738.835657	70042.532772	33.017869
739.335354	70162.211388	33.022887
739.956023	70287.750691	33.027904
741.103591	70420.405175	33.032922
741.601028	70536.153611	33.037940
742.916910	70656.452625	33.042957
743.636451	70788.206399	33.047975
744.643153	70897.935676	33.052992
745.472105	71018.007334	33.058010
746.357097	71137.103023	33.063028
747.027354	71248.577861	33.068045
747.706613	71378.451406	33.073063
748.800528	71482.453399	33.078080
749.467540	71600.304119	33.083098
749.859201	71715.874099	33.088116
750.923044	71832.629921	33.093133
751.709585	71943.494820	33.098151
752.178070	72061.842452	33.103168
753.393482	72184.746508	33.108186
753.806422	72313.101573	33.113204
754.660383	72413.138831	33.118221
755.175829	72541.718617	33.123239
756.006259	72663.645660	33.128256
756.639943	72781.748668	33.133274
756.976008	72917.195818	33.138292
757.791187	73033.575580	33.143309
758.434269	73154.429752	33.148327
759.114965	73291.339964	33.153344
759.792580	73426.354504	33.158362
760.418355	73567.360516	33.163380
761.262624	73703.285151	33.168397
761.845555	73838.254666	33.173415
762.357761	73970.662976	33.178432
763.259621	74119.139496	33.183450
763.938589	74265.592304	33.188468
764.799017	74406.539738	33.193485
765.633880	74541.857785	33.198503
766.198992	74677.904198	33.203520
767.208911	74828.966840	33.208538
767.874052	74974.452831	33.213556
768.895171	75107.441725	33.218573
769.783320	75264.902082	33.223591
770.502508	75389.708673	33.228608
771.762618	75507.912826	33.233626
772.565931	75633.105336	33.238644
773.655266	75763.867199	33.243661
774.300552	75886.778935	33.248679
775.363800	76009.027863	33.253696
776.406707	76125.582655	33.258714
777.030290	76242.308503	33.263732
778.005016	76354.372862	33.268749
778.535571	76458.751131	33.273767
779.429196	76571.158859	33.278784
779.979004	76684.661147	33.283802
780.138402	76803.205853	33.288820
780.981407	76912.866217	33.293837
781.597464	77033.815963	33.298855
782.768484	77171.959804	33.303872
783.441321	77288.594534	33.308890
784.044132	77420.338385	33.313908
784.684973	77553.101343	33.318925
785.639195	77682.530815	33.323943
786.187890	77815.860820	33.328960
787.103496	77936.367590	33.333978
787.938036	78073.813667	33.338996
788.965117	78189.167636	33.344013
789.739889	78325.227347	33.349031
790.374432	78465.327393	33.354048
791.313228	78578.775185	33.359066
792.143704	78720.172732	33.364084
792.660382	78846.297372	33.369101
793.831701	78977.071098	33.374119
794.542021	79119.022331	33.379136
795.372483	79253.098761	33.384154
795.899026	79382.640405	33.389172
796.610075	79509.565308	33.394189
797.446110	79653.801577	33.399207
798.141058	79801.287994	33.404224
799.518668	79920.615974	33.409242
800.172544	80066.580185	33.414260
800.834735	80202.834417	33.419277
801.620806	80332.926978	33.424295
801.992573	80467.978334	33.429312
803.009979	80619.129968	33.434330
803.591727	80761.606253	33.439348
804.502759	80908.596179	33.444365
805.624930	81048.125850	33.449383
806.214574	81194.519170	33.454400
807.059365	81334.868159	33.459418
807.445512	81488.211048	33.464436
808.328443	81630.067443	33.469453
809.180074	81769.526062	33.474471
809.974613	81924.031692	33.479488
811.177478	82072.752275	33.484506
811.646392	82212.390690	33.489524
812.572985	82358.153914	33.494541
813.142443	82522.038039	33.499559
813.947917	82676.034577	33.504576
815.095185	82822.675309	33.509594
815.961713	82977.277445	33.514612
816.772658	83129.738880	33.519629
817.231262	83276.856854	33.524647
818.033435	83434.768726	33.529664
819.140093	83577.289919	33.534682
819.971892	83727.025231	33.539700
821.192913	83866.948165	33.544717
822.227257	84023.408640	33.549735
822.883785	84159.909041	33.554752
823.663454	84299.085046	33.559770
824.917082	84439.006094	33.564788
825.499867	84584.220307	33.569805
826.474359	84723.885505	33.574823
827.327715	84857.206854	33.579840
828.458619	84986.174611	33.584858
829.287828	85129.978669	33.589876
830.050633	85253.896644	33.594893
831.001526	85376.000045	33.599911
831.069332	85520.780069	33.604928
832.045742	85644.936929	33.609946
833.235371	85777.607013	33.614964
833.788377	85902.290714	33.619981
834.634744	86027.356886	33.624999
835.387793	86170.104394	33.630016
835.909891	86309.259141	33.635034
836.879755	86447.069023	33.640052
837.400846	86580.385579	33.645069
838.022547	86709.345796	33.650087
839.024409	86862.958326	33.655104
839.907585	87017.078671	33.660122
841.017791	87150.307543	33.665140
841.926272	87293.669021	33.670157
843.065664	87425.489964	33.675175
843.703202	87577.129923	33.680192
844.663984	87713.392237	33.685210
845.251789	87869.237447	33.690228
846.393968	88003.123971	33.695245
847.534548	88137.043164	33.700263
847.811273	88286.482003	33.705280
848.642604	88432.210763	33.710298
849.638364	88574.825333	33.715316
850.429948	88735.597276	33.720333
851.438476	88875.072974	33.725351
851.698355	89030.176398	33.730368
852.539103	89186.513789	33.735386
853.624252	89333.971707	33.740404
854.263474	89489.224332	33.745421
855.429440	89640.708081	33.750439
856.049866	89797.206125	33.755456
856.948359	89940.458836	33.760474
858.050538	90102.232933	33.765492
858.490834	90257.434844	33.770509
859.532872	90412.418172	33.775527
860.190534	90578.401253	33.780544
861.878893	90728.002129	33.785562
862.752285	90886.901988	33.790580
863.794685	91048.996160	33.795597
864.699614	91184.895365	33.800615
864.997601	91344.494484	33.805632
866.045776	91495.541196	33.810650
867.011795	91646.532812	33.815668
868.077774	91796.110254	33.820685
868.955920	91952.915317	33.825703
869.705214	92099.705380	33.830720
870.779828	92244.404774	33.835738
871.447864	92405.570005	33.840756
872.333608	92554.580700	33.845773
873.103396	92696.795297	33.850791
873.920714	92863.179226	33.855808
875.169975	93011.563123	33.860826
875.980898	93160.722826	33.865844
876.619990	93329.715287	33.870861
877.572009	93473.094220	33.875879
878.310758	93636.812931	33.880896
879.128291	93797.386819	33.885914
879.844120	93936.775838	33.890932
880.769970	94105.650408	33.895949
881.628843	94262.600236	33.900967
882.361744	94425.996111	33.905984
883.192712	94599.351929	33.911002
884.144071	94755.257978	33.916020
884.580852	94924.016435	33.921037
885.747106	95091.864425	33.926055
886.202314	95266.375690	33.931072
886.979156	95426.713849	33.936090
888.235994	95590.638638	33.941108
888.547224	95762.968181	33.946125
889.619388	95907.905017	33.951143
890.600224	96082.056786	33.956160
891.299001	96239.596416	33.961178
892.545215	96408.693506	33.966196
893.354505	96571.622666	33.971213
894.359148	96727.298243	33.976231
895.375657	96888.169714	33.981248
896.583388	97054.865882	33.986266
898.035250	97195.164694	33.991284
899.171588	97352.310013	33.996301
899.939669	97504.548014	34.001319
900.391644	97660.067507	34.006336
901.527746	97805.334088	34.011354
902.394178	97955.431677	34.016372
902.710043	98127.928855	34.021389
903.696748	98280.578625	34.026407
904.947096	98459.203441	34.031424
905.836685	98615.289673	34.036442
906.637284	98770.258429	34.041460
907.113002	98951.325264	34.046477
908.216535	99107.138682	34.051495
908.776152	99290.321158	34.056512
909.480103	99470.062622	34.061530
910.536391	99625.899722	34.066548
911.253406	99808.787770	34.071565
912.177372	99993.896711	34.076583
913.185304	100175.891073	34.081600
913.951270	100364.320815	34.086618
915.626435	100531.064277	34.091636
916.162775	100724.871529	34.096653
917.589066	100888.891839	34.101671
918.365664	101068.303477	34.106688
919.176830	101234.789046	34.111706
920.144393	101412.525518	34.116724
920.679642	101604.566962	34.121741
921.817851	101779.992290	34.126759
922.453264	101955.691779	34.131776
923.376202	102152.010208	34.136794
924.583744	102329.289253	34.141812
925.509720	102515.093683	34.146829
926.435426	102704.445085	34.151847
927.207820	102893.588934	34.156864
928.035520	103066.611421	34.161882
929.208265	103259.712353	34.166900
929.706122	103459.238745	34.171917
931.141757	103643.618559	34.176935
932.446225	103824.950490	34.181952
933.497157	103996.935631	34.186970
935.179117	104158.288028	34.191988
935.668839	104339.948045	34.197005
936.860542	104497.844033	34.202023
938.055532	104668.733439	34.207040
938.529264	104855.072622	34.212058
939.565333	105016.290056	34.217076
940.048969	105183.703744	34.222093
940.914470	105378.625165	34.227111
941.894950	105559.066564	34.232128
942.782639	105734.180211	34.237146
943.541533	105906.796090	34.242164
944.292618	106110.252296	34.247181
945.179409	106298.376249	34.252199
946.162601	106463.448690	34.257216
946.919354	106665.958419	34.262234
947.820210	106853.324137	34.267252
948.930887	107052.510884	34.272269
949.843732	107217.802306	34.277287
950.935177	107398.440656	34.282304
951.831228	107586.230315	34.287322
952.822814	107758.059998	34.292340
953.676464	107926.557260	34.297357
954.917680	108091.850585	34.302375
955.905333	108282.099798	34.307392
956.485155	108466.414225	34.312410
957.780822	108638.655358	34.317428
958.702069	108817.203631	34.322445
959.450218	108987.067592	34.327463
960.979555	109151.889288	34.332480
962.381374	109331.514249	34.337498
963.523672	109493.628103	34.342516
964.209351	109665.558585	34.347533
965.010441	109840.498339	34.352551
966.045107	110012.791409	34.357568
967.074890	110188.404981	34.362586
967.751941	110364.774591	34.367604
968.550832	110548.611168	34.372621
969.765998	110724.374954	34.377639
970.691168	110915.463828	34.382656
971.207654	111101.288796	34.387674
972.679852	111263.206823	34.392692
973.675016	111445.953069	34.397709
974.784824	111634.812473	34.402727
975.718854	111806.031543	34.407744
976.949420	111993.999469	34.412762
977.845452	112167.633857	34.417780
978.598602	112342.749689	34.422797
979.662802	112534.042321	34.427815
980.824617	112722.368631	34.432832
981.502748	112905.227661	34.437850
982.556716	113086.873094	34.442868
983.342561	113278.976942	34.447885
984.018194	113461.789414	34.452903
985.346957	113659.164802	34.457920
985.851494	113860.858151	34.462938
986.945599	114048.951357	34.467956
987.953612	114250.159039	34.472973
988.539340	114454.693670	34.477991
989.664226	114650.399562	34.483008
990.516888	114856.425963	34.488026
991.860918	115046.321607	34.493044
992.819011	115262.101118	34.498061
993.687671	115449.531579	34.503079
994.858734	115652.736827	34.508096
995.808543	115860.325545	34.513114
996.476776	116062.387890	34.518132
997.575108	116277.569299	34.523149
998.556688	116488.464077	34.528167
999.826665	116681.106934	34.533184
1000.667007	116890.254327	34.538202
1002.090620	117088.373149	34.543220
1003.510010	117286.734782	34.548237
1004.711949	117487.477607	34.553255
1005.976981	117683.282878	34.558272
1006.452776	117868.729124	34.563290
1007.785735	118072.735962	34.568308
1008.640731	118266.332350	34.573325
1009.583721	118456.722644	34.578343
1010.440607	118661.990624	34.583360
1011.243149	118861.770123	34.588378
1012.653838	119054.279152	34.593396
1013.576909	119254.915754	34.598413
1014.406959	119453.554490	34.603431
1015.199157	119664.630795	34.608448
1015.588062	119875.091006	34.613466
1016.556817	120074.648766	34.618484
1017.719091	120273.808497	34.623501
1018.483866	120477.368725	34.628519
1019.558502	120679.219308	34.633536
1020.195876	120890.836976	34.638554
1021.494595	121081.857479	34.643572
1022.205007	121292.731078	34.648589
1023.388009	121510.294761	34.653607
1024.281688	121718.834973	34.658624
1024.955686	121935.966326	34.663642
1025.727924	122159.089495	34.668660
1027.062427	122376.115066	34.673677
1028.284160	122594.744856	34.678695
1029.309817	122821.822893	34.683712
1030.174294	123052.122676	34.688730
1031.502836	123257.864840	34.693748
1032.769790	123482.728501	34.698765
1033.667971	123697.377402	34.703783
1035.177870	123909.506413	34.708800
1036.017817	124137.398237	34.713818
1037.025399	124357.609807	34.718836
1038.495332	124576.593448	34.723853
1039.329813	124791.374816	34.728871
1040.788771	125010.895718	34.733888
1041.739542	125219.996136	34.738906
1043.237183	125427.879816	34.743924
1044.300042	125640.639883	34.748941
1045.254903	125864.280352	34.753959
1046.979727	126043.324251	34.758976
1048.173028	126244.876413	34.763994
1049.679131	126437.227938	34.769012
1050.478512	126632.599634	34.774029
1051.495113	126838.341889	34.779047
1052.204037	127027.964501	34.784064
1053.012030	127234.542332	34.789082
1054.414735	127443.697602	34.794100
1055.450263	127653.383868	34.799117
1055.980816	127861.342529	34.804135
1057.586284	128071.850117	34.809152
1058.291797	128285.384807	34.814170
1059.163721	128498.183740	34.819188
1060.188211	128712.289787	34.824205
1060.951670	128932.093303	34.829223
1062.086513	129139.504570	34.834240
1062.758014	129375.321923	34.839258
1064.013524	129586.252541	34.844276
1065.027829	129810.228956	34.849293
1065.826049	130044.091203	34.854311
1066.905402	130274.651274	34.859328
1068.138355	130510.828192	34.864346
1069.028702	130735.693649	34.869364
1070.047766	130962.706977	34.874381
1071.079302	131191.862061	34.879399
1072.529825	131425.373450	34.884416
1073.362781	131668.786877	34.889434
1074.841128	131896.770547	34.894452
1075.726253	132123.193252	34.899469
1076.566898	132356.431944	34.904487
1078.065240	132582.338393	34.909504
1078.890393	132802.475828	34.914522
1079.881761	133052.465373	34.919540
1080.751847	133283.829924	34.924557
1082.146434	133519.584365	34.929575
1083.539724	133734.690620	34.934592
1085.002299	133964.580544	34.939610
1086.566501	134171.168155	34.944628
1087.568245	134376.709034	34.949645
1088.613016	134612.732094	34.954663
1089.637799	134821.428560	34.959680
1090.629031	135028.724759	34.964698
1091.616581	135242.171317	34.969716
1092.660924	135428.569349	34.974733
1092.990222	135656.059584	34.979751
1094.096551	135875.525106	34.984768
1095.322664	136095.301949	34.989786
1095.942839	136308.182278	34.994804
1096.949993	136524.410400	34.999821
1097.870022	136769.762452	35.004839
1099.108465	137004.617225	35.009856
1099.872297	137231.260656	35.014874
1100.914296	137473.073356	35.019892
1102.105358	137704.631979	35.024909
1102.830686	137960.104144	35.029927
1104.507886	138186.324428	35.034944
1105.493841	138433.883994	35.039962
1106.328946	138683.346722	35.044980
1107.762097	138924.864548	35.049997
1108.572421	139175.374689	35.055015
1109.751859	139432.431412	35.060032
1110.874850	139683.603750	35.065050
1112.024296	139936.447222	35.070068
1113.436642	140194.726547	35.075085
1114.290307	140446.405481	35.080103
1115.452609	140686.154883	35.085120
1116.461143	140943.454212	35.090138
1117.368096	141210.991886	35.095156
1118.714326	141463.890358	35.100173
1119.629357	141729.085053	35.105191
1121.081269	141991.428995	35.110208
1122.452698	142262.233000	35.115226
1123.293402	142516.059568	35.120244
1124.787269	142759.686894	35.125261
1125.537519	143036.597182	35.130279
1126.693143	143302.182738	35.135296
1128.432956	143547.791174	35.140314
1129.267445	143802.744083	35.145332
1130.746403	144078.768894	35.150349
1131.552328	144338.409540	35.155367
1132.905793	144586.574476	35.160384
1133.884408	144856.652022	35.165402
1135.170940	145118.438248	35.170420
1136.216715	145373.887638	35.175437
1137.194628	145644.985826	35.180455
1138.356688	145903.057509	35.185472
1139.822337	146168.968692	35.190490
1140.619312	146443.298529	35.195508
1141.929537	146709.505719	35.200525
1142.927271	146983.311994	35.205543
1144.451414	147240.953158	35.210560
1145.701787	147495.534346	35.215578
1146.680121	147759.115601	35.220596
1148.086504	148015.158484	35.225613
1148.995110	148292.565742	35.230631
1150.007040	148551.607080	35.235648
1151.169068	148830.206781	35.240666
1151.870211	149097.698924	35.245684
1153.372774	149357.273759	35.250701
1154.362363	149631.748233	35.255719
1155.514941	149896.863495	35.260736
1156.670079	150172.164416	35.265754
1158.036382	150449.905674	35.270772
1159.528269	150717.405922	35.275789
1160.776869	150976.006801	35.280807
1161.747210	151243.837919	35.285824
1163.018777	151509.262185	35.290842
1163.829784	151780.218142	35.295860
1165.230660	152032.662557	35.300877
1166.088062	152296.537321	35.305895
1167.109426	152558.585823	35.310912
1168.122869	152816.667504	35.315930
1168.950085	153088.809797	35.320948
1169.873073	153347.138339	35.325965
1171.224676	153626.795491	35.330983
1172.362419	153898.384981	35.336000
1173.333497	154165.310838	35.341018
1174.568542	154441.429004	35.346036
1175.990520	154714.664363	35.351053
1176.954897	154995.156501	35.356071
1177.837137	155269.778694	35.361088
1179.435431	155554.812741	35.366106
1181.109200	155838.504551	35.371124
1182.125883	156114.645375	35.376141
1182.825127	156402.383663	35.381159
1184.258171	156683.876174	35.386176
1185.393567	156972.358492	35.391194
1186.623768	157246.505904	35.396212
1188.179956	157540.237951	35.401229
1189.012522	157822.459307	35.406247
1190.056671	158118.994807	35.411264
1191.219519	158410.210440	35.416282
1192.301184	158707.835082	35.421300
1193.534159	159008.151680	35.426317
1194.889106	159310.162961	35.431335
1195.968438	159590.085361	35.436352
1197.452364	159885.686055	35.441370
1198.574264	160186.435733	35.446388
1199.964036	160480.331028	35.451405
1201.051398	160793.206068	35.456423
1202.177682	161082.861294	35.461440
1203.330158	161385.213248	35.466458
1204.449931	161703.075622	35.471476
1206.070404	162001.713865	35.476493
1206.868932	162305.006373	35.481511
1208.008269	162612.710561	35.486528
1209.432153	162914.102790	35.491546
1210.352755	163229.891071	35.496564
1211.449180	163538.243523	35.501581
1212.827788	163854.316150	35.506599
1214.036176	164169.683394	35.511616
1215.500841	164478.299135	35.516634
1216.296161	164807.187811	35.521652
1217.467660	165110.705480	35.526669
1218.778449	165427.054793	35.531687
1220.445620	165744.755950	35.536704
1221.766322	166059.623847	35.541722
1223.127732	166369.945091	35.546740
1224.315921	166681.680139	35.551757
1225.542709	166990.213683	35.556775
1226.873120	167301.612508	35.561792
1228.345135	167616.974273	35.566810
1229.681152	167924.417900	35.571828
1231.591719	168204.818783	35.576845
1232.775607	168502.940254	35.581863
1234.131396	168805.235264	35.586880
1235.526153	169095.420972	35.591898
1236.412265	169408.164202	35.596916
1237.613455	169708.333790	35.601933
1238.972840	169982.276781	35.606951
1239.781446	170278.010437	35.611968
1241.465559	170582.636110	35.616986
1242.355808	170883.550068	35.622004
1243.934804	171171.472809	35.627021
1244.970489	171492.263448	35.632039
1246.111368	171786.721233	35.637056
1247.573841	172071.623438	35.642074
1248.621526	172371.544127	35.647092
1249.437689	172654.475534	35.652109
1250.469421	172938.261366	35.657127
1251.449574	173228.706877	35.662144
1252.662257	173518.900092	35.667162
1253.986034	173829.025321	35.672180
1255.251092	174120.038461	35.677197
1256.300015	174433.042913	35.682215
1257.572649	174731.088880	35.687232
1259.179482	175041.936777	35.692250
1259.973610	175359.443675	35.697268
1261.213286	175659.632874	35.702285
1262.411098	175968.676135	35.707303
1263.565793	176291.320103	35.712320
1264.748193	176609.202656	35.717338
1266.152028	176926.847694	35.722356
1267.913794	177249.892783	35.727373
1269.531713	177550.995792	35.732391
1270.842108	177850.793475	35.737408
1272.358097	178166.575170	35.742426
1273.800392	178471.101314	35.747444
1274.721854	178783.482320	35.752461
1276.160453	179096.097215	35.757479
1277.300479	179399.244813	35.762496
1278.783517	179711.183573	35.767514
1280.219390	180029.439744	35.772532
1281.260714	180337.305152	35.777549
1282.704146	180661.465649	35.782567
1283.716268	180978.972758	35.787584
1284.970552	181283.597718	35.792602
1286.184761	181618.222123	35.797620
1287.148844	181939.652215	35.802637
1288.545116	182263.119857	35.807655
1289.902548	182590.289344	35.812672
1291.377896	182915.131431	35.817690
1292.328381	183256.942955	35.822708
1293.626465	183577.376080	35.827725
1295.011205	183923.321434	35.832743
1296.051607	184253.739399	35.837760
1297.425093	184591.098084	35.842778
1298.653553	184941.797503	35.847796
1299.729207	185274.221394	35.852813
1301.264001	185613.273393	35.857831
1302.310178	185954.870590	35.862848
1304.043476	186296.953092	35.867866
1305.557532	186647.045199	35.872884
1306.790731	186985.977785	35.877901
1307.605923	187329.017902	35.882919
1308.755800	187682.311909	35.887936
1310.206509	188032.905569	35.892954
1311.155729	188387.620728	35.897972
1312.819277	188732.357292	35.902989
1314.676654	189088.983329	35.908007
1315.634454	189442.002719	35.913024
1317.211878	189775.411594	35.918042
1318.161340	190144.710179	35.923060
1319.107565	190488.623672	35.928077
1320.855447	190839.477485	35.933095
1322.120807	191203.767285	35.938112
1323.968070	191554.608985	35.943130
1325.227440	191900.852911	35.948148
1326.599864	192255.509262	35.953165
1328.317018	192596.032690	35.958183
1329.770009	192951.086097	35.963200
1330.970833	193293.882157	35.968218
1332.286427	193647.438986	35.973236
1333.379659	193986.613348	35.978253
1334.998045	194323.824088	35.983271
1335.694572	194668.132922	35.988288
1337.077094	194988.844809	35.993306
1338.415716	195318.375935	35.998324
1339.578529	195677.365008	36.003341
1340.934123	196008.953573	36.008359
1342.113842	196345.498653	36.013376
1343.234367	196685.330671	36.018394
1344.354336	197039.243739	36.023412
1345.763787	197393.771148	36.028429
1347.303315	197747.225313	36.033447
1348.278141	198103.770758	36.038464
1349.572149	198464.734337	36.043482
1351.035476	198828.718929	36.048500
1351.971247	199191.865806	36.053517
1353.187818	199565.340831	36.058535
1354.098581	199934.247104	36.063552
1355.982316	200307.984346	36.068570
1356.902134	200685.551900	36.073588
1358.585168	201060.989603	36.078605
1360.321752	201428.282269	36.083623
1361.532305	201824.382657	36.088640
1363.254877	202187.314158	36.093658
1364.335177	202563.811730	36.098676
1365.725488	202956.587818	36.103693
1367.414669	203339.400767	36.108711
1368.457439	203734.866707	36.113728
1369.575137	204117.282976	36.118746
1370.712522	204514.146919	36.123764
1372.228247	204911.623522	36.128781
1373.808265	205302.730535	36.133799
1374.884597	205711.673091	36.138816
1376.322798	206104.788477	36.143834
1377.653772	206508.627272	36.148852
1378.765783	206915.323138	36.153869
1380.516752	207317.865319	36.158887
1381.687209	207734.688300	36.163904
1383.133694	208140.053054	36.168922
1384.881206	208545.789259	36.173940
1385.915051	208952.673846	36.178957
1387.744214	209356.292980	36.183975
1389.370046	209761.293669	36.188992
1391.264418	210157.249430	36.194010
1392.979428	210558.633276	36.199028
1394.465600	210949.809737	36.204045
1396.023127	211347.452201	36.209063
1397.302291	211753.180305	36.214080
1398.906980	212118.819904	36.219098
1400.681542	212501.169079	36.224116
1401.690414	212907.772738	36.229133
1403.332157	213280.115835	36.234151
1404.512309	213679.837883	36.239168
1405.787971	214077.692061	36.244186
1407.305160	214460.574950	36.249204
1408.384401	214862.376181	36.254221
1410.197072	215264.743902	36.259239
1410.875581	215653.687804	36.264256
1412.661699	216054.920567	36.269274
1413.831528	216449.907492	36.274292
1415.006625	216856.755792	36.279309
1416.817428	217248.821240	36.284327
1417.683796	217655.596977	36.289344
1419.381922	218059.392656	36.294362
1420.822902	218464.807138	36.299380
1421.985866	218875.983721	36.304397
1423.894450	219275.228930	36.309415
1425.334088	219721.158626	36.314432
1426.342904	220161.015050	36.319450
1427.422958	220565.659589	36.324468
1428.516990	220954.048456	36.329485
1430.125709	221353.808575	36.334503
1431.923686	221754.478750	36.339520
1432.935462	222149.235313	36.344538
1434.306158	222551.858537	36.349556
1435.361088	222956.389503	36.354573
1437.233091	223357.256687	36.359591
1438.078785	223787.503637	36.364608
1439.597286	224186.908239	36.369626
1441.002168	224606.296832	36.374644
1442.230384	225029.983226	36.379661
1443.557867	225447.635139	36.384679
1445.266615	225873.531288	36.389696
1446.769721	226305.457233	36.394714
1448.426790	226743.150480	36.399732
1449.974025	227164.582165	36.404749
1451.577074	227569.851765	36.409767
1452.734287	228022.821240	36.414784
1454.289657	228458.530799	36.419802
1455.850681	228877.959421	36.424820
1457.404128	229310.827394	36.429837
1459.700373	229727.445023	36.434855
1460.371575	230151.469650	36.439872
1461.939740	230589.190871	36.444890
1463.751735	231005.816196	36.449908
1464.994393	231442.654047	36.454925
1466.751626	231881.008597	36.459943
1468.027771	232314.058922	36.464960
1469.734974	232753.034025	36.469978
1471.289479	233179.843188	36.474996
1472.251121	233619.578932	36.480013
1473.841819	234057.129262	36.485031
1474.994946	234495.007060	36.490048
1476.328109	234945.887218	36.495066
1478.009972	235394.679011	36.500084
1479.211424	235850.638316	36.505101
1481.036245	236311.169888	36.510119
1482.529353	236756.364142	36.515136
1484.203094	237214.001931	36.520154
1485.518623	237654.274500	36.525172
1486.905981	238119.023569	36.530189
1488.489072	238567.027159	36.535207
1490.512168	239022.224156	36.540224
1492.649332	239454.846540	36.545242
1494.358239	239891.020636	36.550260
1496.059677	240323.539045	36.555277
1497.446780	240760.301600	36.560295
1498.858586	241195.587687	36.565312
1500.722569	241638.192098	36.570330
1502.406296	242080.547744	36.575348
1503.571453	242524.945830	36.580365
1504.968683	242948.883027	36.585383
1506.016932	243396.147169	36.590400
1507.592435	243831.233601	36.595418
1509.297498	244258.297659	36.600436
1510.353399	244713.640958	36.605453
1511.964785	245155.582467	36.610471
1513.135823	245610.705124	36.615488
1514.774839	246064.836830	36.620506
1516.343696	246498.988942	36.625524
1517.887429	246960.250558	36.630541
1519.655873	247403.973310	36.635559
1521.697775	247845.111301	36.640576
1522.335910	248304.187314	36.645594
1523.813421	248747.121657	36.650612
1525.491752	249204.223656	36.655629
1527.251646	249652.650387	36.660647
1528.323135	250106.449669	36.665664
1529.476384	250537.093873	36.670682
1531.409022	250988.389598	36.675700
1532.640354	251421.562147	36.680717
1534.354259	251843.732176	36.685735
1536.060422	252292.475500	36.690752
1537.411272	252724.765847	36.695770
1539.213075	253157.185373	36.700788
1540.252697	253597.148732	36.705805
1542.419723	254046.528797	36.710823
1543.724276	254497.169246	36.715840
1544.855606	254932.444245	36.720858
1546.813462	255395.856914	36.725876
1547.772207	255849.248026	36.730893
1549.179431	256290.575048	36.735911
1550.962689	256759.224947	36.740928
1552.476892	257222.533961	36.745946
1554.130283	257682.365346	36.750964
1555.158370	258154.392032	36.755981
1556.983543	258628.980083	36.760999
1558.623942	259085.943445	36.766016
1559.742548	259576.017285	36.771034
1561.430220	260052.939993	36.776052
1562.837483	260544.541312	36.781069
1563.662670	261033.469727	36.786087
1565.682640	261531.905042	36.791104
1567.134577	262032.212266	36.796122
1568.537471	262535.677511	36.801140
1569.785211	263051.412631	36.806157
1571.521785	263550.300773	36.811175
1573.538616	264075.333275	36.816192
1574.722767	264574.972667	36.821210
1576.355472	265082.514430	36.826228
1577.676512	265608.905738	36.831245
1579.497022	266129.600190	36.836263
1580.845380	266647.654046	36.841280
1582.644341	267184.279096	36.846298
1584.747078	267695.704442	36.851316
1586.297573	268229.778445	36.856333
1587.827937	268748.892815	36.861351
1589.549997	269265.333105	36.866368
1590.824999	269797.139239	36.871386
1592.660625	270325.372028	36.876404
1594.159370	270852.338792	36.881421
1595.830956	271375.211875	36.886439
1597.444256	271903.758713	36.891456
1599.283939	272428.838045	36.896474
1601.365134	272939.422521	36.901492
1603.431001	273470.153169	36.906509
1604.686582	273983.056881	36.911527
1606.507291	274497.416061	36.916544
1607.872173	275038.166727	36.921562
1609.539810	275542.489858	36.926580
1610.957739	276065.676577	36.931597
1612.215269	276589.625406	36.936615
1614.579976	277117.150056	36.941632
1615.737347	277651.833056	36.946650
1617.827095	278166.293169	36.951668
1618.899014	278709.548485	36.956685
1620.274066	279235.910800	36.961703
1622.109518	279761.281417	36.966720
1623.399234	280294.259819	36.971738
1625.086389	280824.707286	36.976756
1626.495681	281371.812111	36.981773
1628.284875	281924.872995	36.986791
1630.307264	282452.974612	36.991808
1631.573145	282998.040936	36.996826
1633.458895	283525.755618	37.001844
1635.189921	284054.942166	37.006861
1636.364162	284576.319102	37.011879
1638.158565	285092.029208	37.016896
1639.261428	285623.880099	37.021914
1641.083426	286145.526299	37.026932
1642.765166	286678.497487	37.031949
1644.142377	287202.093297	37.036967
1645.925382	287733.850315	37.041984
1647.247992	288271.853855	37.047002
1649.431963	288796.530282	37.052020
1650.737913	289336.082125	37.057037
1652.864735	289862.161144	37.062055
1654.375758	290387.323765	37.067072
1655.991651	290934.463891	37.072090
1657.760037	291468.292251	37.077108
1659.531041	292003.337246	37.082125
1660.599935	292553.786786	37.087143
1662.927529	293098.590684	37.092160
1664.072038	293659.182986	37.097178
1665.934600	294200.502818	37.102196
1667.461387	294756.201084	37.107213
1669.117050	295311.113526	37.112231
1670.788001	295862.693508	37.117248
1672.406823	296431.982818	37.122266
1674.197602	296979.854781	37.127284
1676.181025	297550.018101	37.132301
1677.992791	298103.976874	37.137319
1680.085320	298653.492517	37.142336
1681.240666	299222.437593	37.147354
1683.279399	299778.915569	37.152372
1684.876864	300344.556024	37.157389
1686.297528	300917.969022	37.162407
1688.121630	301475.997143	37.167424
1689.694155	302038.813089	37.172442
1691.147634	302625.722638	37.177460
1692.667693	303203.169724	37.182477
1694.415800	303782.251957	37.187495
1696.448542	304368.090194	37.192512
1698.087382	304949.824605	37.197530
1699.894897	305530.181479	37.202548
1701.307689	306113.215660	37.207565
1702.810553	306696.485170	37.212583
1704.748103	307283.387036	37.217600
1706.252316	307888.489494	37.222618
1707.973987	308477.679211	37.227636
1709.412525	309081.946037	37.232653
1710.672751	309707.189536	37.237671
1712.268594	310304.259978	37.242688
1713.736283	310931.771017	37.247706
1715.478037	311536.528621	37.252724
1717.247347	312166.519843	37.257741
1719.082504	312791.974913	37.262759
1720.852591	313399.634060	37.267776
1722.587269	314036.904246	37.272794
1724.268183	314653.507068	37.277812
1726.526242	315268.562192	37.282829
1728.249048	315901.577835	37.287847
1730.200098	316526.652989	37.292864
1731.674705	317143.396185	37.297882
1733.214304	317775.917970	37.302900
1735.030994	318400.338881	37.307917
1736.770528	319032.918083	37.312935
1738.509324	319662.241450	37.317952
1740.196126	320283.899209	37.322970
1741.858402	320910.633786	37.327988
1743.818374	321544.220033	37.333005
1745.698556	322179.819395	37.338023
1747.590126	322796.494258	37.343040
1749.497118	323418.721443	37.348058
1750.896715	324012.334725	37.353076
1753.070785	324630.443676	37.358093
1754.780715	325225.949614	37.363111
1756.948008	325823.431097	37.368128
1758.714356	326419.906654	37.373146
1760.233202	327017.559850	37.378164
1762.506921	327594.593463	37.383181
1763.790204	328194.863761	37.388199
1765.536870	328800.713384	37.393216
1767.267773	329410.088506	37.398234
1768.830981	330021.262230	37.403252
1770.626657	330633.457562	37.408269
1771.804763	331240.823111	37.413287
1773.636369	331863.180090	37.418304
1775.235972	332508.823352	37.423322
1776.639475	333138.421658	37.428340
1778.708951	333763.104976	37.433357
1780.349937	334414.355431	37.438375
1782.029844	335050.690149	37.443392
1783.578390	335687.521491	37.448410
1785.519522	336346.924517	37.453428
1787.571268	336990.993947	37.458445
1789.260603	337647.985560	37.463463
1790.829266	338302.856636	37.468480
1792.358790	338975.698082	37.473498
1793.683598	339630.313559	37.478516
1795.548955	340311.002092	37.483533
1797.181076	340989.790933	37.488551
1799.456048	341661.433586	37.493568
1801.229323	342343.937655	37.498586
1803.210669	343022.946093	37.503604
1805.520620	343699.124392	37.508621
1807.327842	344380.884118	37.513639
1809.238038	345059.267006	37.518656
1811.130005	345731.247414	37.523674
1812.751107	346413.669089	37.528692
1814.769898	347105.532919	37.533709
1816.459936	347778.456795	37.538727
1818.821168	348460.929827	37.543744
1820.695504	349153.396343	37.548762
1822.331634	349822.644940	37.553780
1824.314649	350508.550795	37.558797
1825.744042	351204.663381	37.563815
1827.737106	351878.010154	37.568832
1829.488034	352569.683611	37.573850
1831.299736	353268.390983	37.578868
1833.388777	353956.865637	37.583885
1834.719748	354663.801258	37.588903
1836.638661	355364.918903	37.593920
1838.357571	356054.131854	37.598938
1839.821466	356766.593555	37.603956
1841.724393	357464.837444	37.608973
1843.507003	358169.356935	37.613991
1845.729234	358887.747382	37.619008
1847.507863	359606.655286	37.624026
1849.258890	360315.685317	37.629044
1851.333698	361026.273463	37.634061
1853.063114	361738.732909	37.639079
1855.294155	362443.714028	37.644096
1856.946383	363150.807873	37.649114
1858.776014	363879.652911	37.654132
1861.196465	364577.385198	37.659149
1863.406983	365290.006119	37.664167
1865.661786	365975.233711	37.669184
1868.028233	366662.257281	37.674202
1869.991522	367352.759749	37.679220
1872.156079	368027.716998	37.684237
1873.794557	368704.854488	37.689255
1875.666165	369361.648092	37.694272
1877.433071	370033.971546	37.699290
1878.804921	370681.261360	37.704308
1880.657992	371340.686541	37.709325
1882.582601	372009.346260	37.714343
1883.746975	372666.578393	37.719360
1885.242003	373343.122110	37.724378
1886.478237	374049.244191	37.729396
1888.714508	374736.723273	37.734413
1890.048656	375433.924907	37.739431
1891.557178	376138.920907	37.744448
1893.081385	376834.465803	37.749466
1894.534592	377574.846608	37.754484
1896.630586	378308.765581	37.759501
1898.231876	379058.752603	37.764519
1899.920225	379794.989588	37.769536
1901.915949	380547.440275	37.774554
1903.695622	381298.210940	37.779572
1905.845368	382058.083288	37.784589
1907.762567	382795.840165	37.789607
1909.916776	383568.989840	37.794624
1912.068371	384334.134833	37.799642
1913.893885	385106.339213	37.804660
1915.927485	385859.855422	37.809677
1917.920190	386635.038583	37.814695
1919.684409	387397.488083	37.819712
1921.736807	388171.534232	37.824730
1923.495912	388947.511400	37.829748
1925.747438	389730.233284	37.834765
1927.758484	390502.733636	37.839783
1929.818554	391287.476397	37.844800
1931.866029	392071.263531	37.849818
1933.928113	392843.215785	37.854836
1936.038553	393609.183837	37.859853
1938.126367	394402.385248	37.864871
1939.792803	395180.452594	37.869888
1942.164861	395960.664716	37.874906
1943.717007	396746.213047	37.879924
1945.795703	397524.379851	37.884941
1947.565621	398320.647769	37.889959
1949.876253	399111.913707	37.894976
1952.031942	399900.548209	37.899994
1953.628383	400687.555718	37.905012
1955.975573	401475.989258	37.910029
1958.022239	402253.934332	37.915047
1960.065125	403040.728052	37.920064
1961.941095	403832.671558	37.925082
1964.014002	404631.148599	37.930100
1966.264127	405404.945144	37.935117
1968.021215	406186.174886	37.940135
1969.984664	406986.630000	37.945152
1972.185729	407773.012044	37.950170
1974.175440	408566.475105	37.955188
1976.434817	409353.258456	37.960205
1978.147525	410138.918628	37.965223
1980.302368	410910.955296	37.970240
1982.767395	411702.779337	37.975258
1984.427028	412489.317266	37.980276
1986.569868	413255.892969	37.985293
1988.384048	414049.097455	37.990311
1990.106500	414837.784682	37.995328
1991.889199	415620.967381	38.000346
1993.697054	416423.321041	38.005364
1995.774246	417213.321959	38.010381
1998.262379	417996.848807	38.015399
2000.312155	418789.186796	38.020416
2002.316211	419579.152671	38.025434
2004.531164	420360.322564	38.030452
2006.561851	421106.654101	38.035469
2008.448811	421870.966278	38.040487
2010.434527	422624.654496	38.045504
2012.308669	423382.643005	38.050522
2014.270022	424142.417145	38.055540
2016.473960	424893.367510	38.060557
2018.264686	425660.237969	38.065575
2019.905023	426438.198517	38.070592
2022.213399	427203.871998	38.075610
2023.791778	427986.806190	38.080628
2025.821385	428753.438835	38.085645
2027.711313	429530.195991	38.090663
2029.128701	430333.484135	38.095680
2031.600941	431132.014998	38.100698
2032.832050	431934.166181	38.105716
2034.815542	432730.850760	38.110733
2037.226909	433549.913384	38.115751
2038.959020	434374.425015	38.120768
2041.065970	435193.783997	38.125786
2043.023333	436016.378117	38.130804
2045.102506	436850.715796	38.135821
2047.147259	437679.917123	38.140839
2048.930403	438513.838264	38.145856
2051.565524	439352.345514	38.150874
2053.412026	440206.032385	38.155892
2055.309859	441035.945199	38.160909
2057.372507	441889.431381	38.165927
2058.914459	442753.192087	38.170944
2061.039613	443608.271977	38.175962
2063.102484	444483.061650	38.180980
2065.392844	445349.734587	38.185997
2067.254712	446224.184541	38.191015
2069.264781	447111.779046	38.196032
2071.527450	447978.503901	38.201050
2073.554800	448864.101408	38.206068
2075.210952	449760.042796	38.211085
2077.387526	450648.577075	38.216103
2079.611486	451545.108652	38.221120
2081.586233	452426.368983	38.226138
2083.700304	453334.172218	38.231156
2085.953254	454232.203243	38.236173
2088.410641	455136.584487	38.241191
2090.311030	456036.214221	38.246208
2092.397755	456943.359131	38.251226
2094.316278	457848.014185	38.256244
2096.521933	458768.407940	38.261261
2098.558808	459669.575267	38.266279
2101.151386	460590.732917	38.271296
2103.076189	461498.056007	38.276314
2105.662151	462403.207040	38.281332
2107.824899	463310.965053	38.286349
2109.968244	464214.085034	38.291367
2111.821201	465128.281424	38.296384
2114.455876	466029.721200	38.301402
2116.462175	466943.353246	38.306420
2118.921472	467849.590328	38.311437
2121.447855	468748.800138	38.316455
2123.182432	469655.577955	38.321472
2125.288408	470563.464744	38.326490
2127.373338	471463.783233	38.331508
2129.433493	472357.090716	38.336525
2131.822818	473255.000887	38.341543
2133.821919	474175.314417	38.346560
2136.257075	475084.649424	38.351578
2138.417859	475972.162117	38.356596
2140.269595	476877.364079	38.361613
2142.887202	477779.415581	38.366631
2144.570970	478673.899709	38.371648
2146.699447	479545.942761	38.376666
2148.516278	480425.925305	38.381684
2150.874411	481296.029286	38.386701
2153.191100	482177.915838	38.391719
2154.727098	483042.668488	38.396736
2157.043171	483917.602908	38.401754
2159.146942	484818.534019	38.406772
2161.332103	485705.723556	38.411789
2163.587159	486590.939055	38.416807
2165.091530	487497.690867	38.421824
2167.131755	488394.817195	38.426842
2169.311764	489307.826852	38.431860
2171.620769	490219.203102	38.436877
2173.790170	491116.724777	38.441895
2175.998395	492051.190471	38.446912
2178.308670	492947.585224	38.451930
2180.628016	493871.285466	38.456948
2182.619955	494794.939802	38.461965
2185.249094	495717.934821	38.466983
2187.058273	496635.918904	38.472000
2189.242564	497566.607676	38.477018
2191.277981	498487.431517	38.482036
2193.561167	499442.622385	38.487053
2195.500092	500375.719602	38.492071
2197.599729	501340.972947	38.497088
2199.887376	502289.594453	38.502106
2201.906041	503251.774443	38.507124
2203.759409	504219.726028	38.512141
2206.033189	505185.181153	38.517159
2208.186914	506152.868743	38.522176
2210.629072	507125.544751	38.527194
2212.534996	508098.503272	38.532212
2215.559069	509076.059582	38.537229
2218.096231	510045.469285	38.542247
2220.329917	511012.904475	38.547264
2222.817613	511981.650982	38.552282
2224.844835	512957.522385	38.557300
2227.856117	513925.963597	38.562317
2230.501546	514887.551122	38.567335
2232.512852	515850.948636	38.572352
2235.075004	516809.156607	38.577370
2237.646780	517772.192580	38.582388
2239.754747	518729.148304	38.587405
2241.914398	519686.137368	38.592423
2244.034809	520653.553744	38.597440
2246.437438	521611.945406	38.602458
2248.774741	522567.567633	38.607476
2250.782626	523531.949782	38.612493
2253.032178	524496.029609	38.617511
2255.481199	525458.655406	38.622528
2257.735727	526422.208980	38.627546
2259.916365	527391.504812	38.632564
2261.848366	528357.606472	38.637581
2264.368847	529327.980029	38.642599
2266.318662	530312.583888	38.647616
2268.259655	531291.031689	38.652634
2270.690839	532275.828555	38.657652
2272.399932	533262.793053	38.662669
2274.865752	534241.512211	38.667687
2276.898103	535251.395053	38.672704
2279.230858	536238.055973	38.677722
2280.964835	537242.615221	38.682740
2283.317232	538242.272175	38.687757
2285.261535	539263.162756	38.692775
2287.314264	540282.101088	38.697792
2289.181358	541305.374767	38.702810
2291.815462	542328.096298	38.707828
2294.023882	543354.184870	38.712845
2296.169752	544345.348955	38.717863
2298.351117	545354.796925	38.722880
2300.604507	546349.675051	38.727898
2302.795534	547368.884639	38.732916
2304.918095	548380.085270	38.737933
2307.165564	549385.911658	38.742951
2309.212139	550404.922085	38.747968
2311.421116	551442.986245	38.752986
2314.156258	552465.652081	38.758004
2316.216845	553499.713734	38.763021
2318.807263	554534.363538	38.768039
2320.439019	555593.319103	38.773056
2322.783162	556633.579103	38.778074
2325.295007	557697.200096	38.783092
2327.156009	558753.356736	38.788109
2329.644059	559818.220251	38.793127
2331.830587	560907.416049	38.798144
2333.851689	561978.664803	38.803162
2336.278808	563065.181796	38.808180
2338.868434	564162.733476	38.813197
2341.674050	565240.469099	38.818215
2343.915789	566344.776208	38.823232
2346.022571	567433.996846	38.828250
2348.309110	568530.126274	38.833268
2350.769214	569646.770058	38.838285
2353.730178	570752.591010	38.843303
2355.844092	571868.195133	38.848320
2357.846079	572971.020724	38.853338
2360.647124	574078.387247	38.858356
2363.220667	575185.594198	38.863373
2366.306870	576296.383309	38.868391
2368.830713	577393.769453	38.873408
2371.247340	578496.496046	38.878426
2373.779094	579609.742293	38.883444
2376.138416	580721.261967	38.888461
2378.838833	581813.865728	38.893479
2381.065025	582927.316035	38.898496
2383.806963	584031.653647	38.903514
2386.303377	585132.321732	38.908532
2388.405960	586243.535724	38.913549
2390.775434	587339.813636	38.918567
2393.241689	588452.570744	38.923584
2395.875067	589562.992238	38.928602
2398.322929	590677.552411	38.933620
2400.572871	591798.356805	38.938637
2402.749598	592909.696799	38.943655
2404.571693	594034.771938	38.948672
2407.078004	595161.782253	38.953690
2409.356743	596290.075477	38.958708
2411.285794	597425.081327	38.963725
2413.653991	598564.513517	38.968743
2416.125221	599725.555123	38.973760
2418.308956	600872.255508	38.978778
2420.862953	602023.188418	38.983796
2422.494307	603187.878499	38.988813
2424.975803	604356.015773	38.993831
2427.329111	605533.516977	38.998848
2430.059455	606705.679269	39.003866
2432.417117	607877.882718	39.008884
2434.728540	609069.690794	39.013901
2437.207293	610255.191025	39.018919
2439.388282	611446.219745	39.023936
2442.014760	612623.140758	39.028954
2444.908914	613816.502065	39.033972
2447.404494	614999.847815	39.038989
2449.941771	616171.607767	39.044007
2452.182251	617369.747129	39.049024
2454.165318	618561.298657	39.054042
2456.714863	619711.630014	39.059060
2459.286492	620875.884908	39.064077
2461.828332	622026.724225	39.069095
2464.176285	623199.765701	39.074112
2465.971776	624364.525464	39.079130
2468.515133	625524.639148	39.084148
2470.518111	626708.850335	39.089165
2472.980281	627907.893196	39.094183
2475.541844	629101.090634	39.099200
2477.487833	630293.606783	39.104218
2480.355210	631484.189195	39.109236
2482.309370	632705.449799	39.114253
2484.819290	633910.799090	39.119271
2487.590994	635136.286872	39.124288
2489.899124	636364.353562	39.129306
2492.193597	637589.532886	39.134324
2494.647077	638827.268342	39.139341
2497.066396	640079.582816	39.144359
2499.465876	641333.844460	39.149376
2501.667582	642597.814240	39.154394
2504.070676	643854.212387	39.159412
2506.509390	645127.857509	39.164429
2509.204876	646403.046586	39.169447
2511.863121	647689.550528	39.174464
2514.304828	648979.665923	39.179482
2517.017470	650256.859251	39.184500
2519.831080	651552.615479	39.189517
2522.622803	652849.553174	39.194535
2525.165876	654131.164169	39.199552
2527.587995	655428.723662	39.204570
2530.765991	656718.116968	39.209588
2533.249768	658012.387648	39.214605
2535.427253	659315.254548	39.219623
2538.083675	660609.851404	39.224640
2540.501156	661919.901220	39.229658
2543.692013	663221.631429	39.234676
2546.085788	664530.834892	39.239693
2548.925497	665823.163102	39.244711
2551.821238	667121.628827	39.249728
2554.083775	668436.742316	39.254746
2556.869065	669729.647622	39.259764
2559.632979	671028.947349	39.264781
2562.188197	672322.632210	39.269799
2565.239161	673620.335330	39.274816
2568.156734	674916.340187	39.279834
2570.948170	676207.911122	39.284852
2573.263230	677516.682017	39.289869
2575.822332	678812.902207	39.294887
2578.544168	680086.202786	39.299904
2580.976545	681379.103406	39.304922
2583.869256	682670.753371	39.309940
2586.271606	683971.393701	39.314957
2588.563747	685273.407453	39.319975
2591.336264	686576.745706	39.324992
2593.677409	687874.556014	39.330010
2596.624471	689161.853209	39.335028
2598.966637	690477.908674	39.340045
2601.072241	691784.579010	39.345063
2604.057542	693081.683658	39.350080
2606.689074	694404.808384	39.355098
2609.191940	695718.182914	39.360116
2611.874909	697028.258277	39.365133
2614.105535	698344.860672	39.370151
2616.941697	699667.217076	39.375168
2619.172667	700993.193329	39.380186
2622.050774	702312.516902	39.385204
2624.206891	703641.475746	39.390221
2627.068879	704957.527299	39.395239
2629.627935	706240.972190	39.400256
2632.107193	707534.000503	39.405274
2634.674362	708817.656038	39.410292
2637.734967	710101.583553	39.415309
2640.041779	711394.406803	39.420327
2643.152222	712684.129188	39.425344
2645.354366	713979.202457	39.430362
2648.260472	715261.983030	39.435380
2651.165045	716558.873057	39.440397
2653.520369	717862.483325	39.445415
2655.924649	719159.797727	39.450432
2658.522954	720471.077428	39.455450
2661.005219	721785.682377	39.460468
2663.598824	723113.513214	39.465485
2666.070250	724438.877335	39.470503
2668.331342	725788.437196	39.475520
2670.984371	727135.833373	39.480538
2673.725754	728474.691259	39.485556
2676.031537	729832.871497	39.490573
2678.468702	731206.367210	39.495591
2681.350884	732576.495276	39.500608
2683.798079	733963.206678	39.505626
2686.384855	735356.076864	39.510644
2688.900144	736748.816954	39.515661
2692.243050	738136.933994	39.520679
2694.998886	739548.794957	39.525696
2697.368419	740955.979368	39.530714
2700.009185	742360.995373	39.535732
2702.808371	743775.947334	39.540749
2705.204125	745190.564481	39.545767
2708.060272	746611.903149	39.550784
2710.470423	748056.328428	39.555802
2713.103228	749488.176474	39.560820
2715.794429	750949.124964	39.565837
2718.502076	752390.776216	39.570855
2721.637506	753844.503402	39.575872
2724.636678	755293.201405	39.580890
2727.537881	756749.275909	39.585908
2730.074669	758205.035437	39.590925
2732.481659	759660.539006	39.595943
2736.004022	761112.676690	39.600960
2738.632948	762580.233709	39.605978
2741.327608	764050.053524	39.610996
2743.773937	765511.265457	39.616013
2746.695230	766980.032928	39.621031
2749.532430	768442.429026	39.626048
2752.029095	769925.537125	39.631066
2754.595348	771409.615963	39.636084
2757.140323	772899.248971	39.641101
2760.154967	774387.816397	39.646119
2763.183918	775870.087742	39.651136
2765.722993	777373.356376	39.656154
2768.474520	778856.100536	39.661172
2771.043404	780369.107726	39.666189
2773.716477	781860.383482	39.671207
2776.668218	783365.732898	39.676224
2779.292890	784872.441153	39.681242
2782.243198	786380.840185	39.686260
2785.211464	787884.554281	39.691277
2788.115983	789399.091980	39.696295
2790.730430	790909.384773	39.701312
2793.198839	792425.604250	39.706330
2796.175274	793932.007380	39.711348
2799.012411	795453.297576	39.716365
2801.549282	796976.168928	39.721383
2804.547990	798485.705937	39.726400
2807.640309	800002.586969	39.731418
2810.746637	801512.820987	39.736436
2813.462916	802976.841015	39.741453
2816.075989	804442.916231	39.746471
2819.532115	805894.257707	39.751488
2822.834498	807344.046214	39.756506
2825.731969	808794.132155	39.761524
2828.778700	810235.624162	39.766541
2831.408812	811690.563536	39.771559
2833.834064	813147.765299	39.776576
2836.374679	814615.723117	39.781594
2838.248469	816079.417288	39.786612
2840.940349	817571.711374	39.791629
2843.393699	819075.526274	39.796647
2846.472257	820577.874374	39.801664
2848.675152	822082.125740	39.806682
2851.727584	823607.556612	39.811700
2854.555709	825127.502357	39.816717
2857.036515	826669.634277	39.821735
2859.974783	828208.403644	39.826752
2862.784836	829763.208903	39.831770
2865.551239	831322.864719	39.836788
2868.580392	832876.159803	39.841805
2870.988173	834446.280290	39.846823
2873.913362	836009.993456	39.851840
2876.536996	837604.142718	39.856858
2879.423858	839203.741514	39.861876
2882.729485	840790.999157	39.866893
2885.123972	842399.804244	39.871911
2888.028153	843999.510220	39.876928
2890.855681	845610.687839	39.881946
2894.026205	847231.605079	39.886964
2896.706271	848862.390213	39.891981
2899.724258	850487.060007	39.896999
2902.623111	852119.000846	39.902016
2905.789005	853757.364956	39.907034
2908.495758	855381.974243	39.912052
2911.320855	857039.914507	39.917069
2913.910717	858693.663284	39.922087
2917.323307	860349.547585	39.927104
2920.306785	861998.459933	39.932122
2922.950218	863653.284865	39.937140
2925.967297	865325.142154	39.942157
2928.830260	866995.982241	39.947175
2932.475517	868654.799926	39.952192
2935.208041	870327.547628	39.957210
2938.296638	871999.479829	39.962228
2941.044589	873658.514123	39.967245
2943.749964	875346.414150	39.972263
2947.059274	877024.641426	39.977280
2949.973049	878707.293628	39.982298
2952.825223	880391.409705	39.987316
2956.207600	882054.754639	39.992333
2959.289205	883751.690519	39.997351
2962.559045	885427.526161	40.002368
2965.374769	887103.340342	40.007386
2967.931453	888778.713060	40.012404
2971.127805	890470.385471	40.017421
2973.759942	892154.224480	40.022439
2976.671032	893832.314921	40.027456
2979.378323	895540.033832	40.032474
2982.106014	897231.910004	40.037492
2985.329835	898937.560760	40.042509
2987.820427	900654.669312	40.047527
2991.027226	902361.987724	40.052544
2993.799029	904064.238052	40.057562
2996.364414	905802.968604	40.062580
2999.557870	907534.800110	40.067597
3002.293823	909268.958308	40.072615
3005.526266	910981.336259	40.077632
3008.292161	912679.801841	40.082650
3010.882639	914369.700157	40.087668
3013.713311	916068.455107	40.092685
3016.485195	917782.252896	40.097703
3019.573993	919479.425504	40.102720
3022.004433	921192.399365	40.107738
3024.586612	922917.857596	40.112756
3027.420853	924641.380650	40.117773
3030.115244	926390.555104	40.122791
3033.044920	928134.615418	40.127808
3036.207281	929904.519021	40.132826
3038.944222	931683.581292	40.137844
3042.192733	933460.814634	40.142861
3044.831379	935241.381639	40.147879
3047.766524	937030.486892	40.152896
3050.943784	938840.948270	40.157914
3054.106054	940649.543626	40.162932
3057.055875	942449.995115	40.167949
3060.126794	944269.109594	40.172967
3063.122124	946102.693762	40.177984
3066.773208	947934.755656	40.183002
3069.511164	949774.049577	40.188020
3072.731894	951608.787718	40.193037
3075.560475	953453.522096	40.198055
3078.565865	955330.785926	40.203072
3081.757745	957236.340576	40.208090
3084.578035	959145.434720	40.213108
3087.704752	961064.111134	40.218125
3090.309822	962995.329868	40.223143
3093.472860	964943.198152	40.228160
3096.104139	966886.685942	40.233178
3099.471549	968852.532566	40.238196
3102.433788	970800.499361	40.243213
3105.289603	972785.870124	40.248231
3108.145825	974764.896923	40.253248
3111.181112	976746.427671	40.258266
3113.995932	978730.524699	40.263284
3117.534439	980728.329984	40.268301
3121.082084	982730.693977	40.273319
3124.474069	984732.478368	40.278336
3128.061838	986730.705396	40.283354
3131.024158	988735.825476	40.288372
3133.975147	990744.909067	40.293389
3137.272403	992754.489556	40.298407
3140.289050	994752.909606	40.303424
3143.502416	996769.148925	40.308442
3146.899360	998781.144935	40.313460
3150.002152	1000801.503128	40.318477
3153.153185	1002823.461204	40.323495
3155.935607	1004846.115079	40.328512
3159.295413	1006873.671157	40.333530
3162.330360	1008907.241147	40.338548
3165.094898	1010924.520510	40.343565
3168.599887	1012964.688728	40.348583
3171.356746	1015012.762000	40.353600
3174.543912	1017062.728740	40.358618
3177.380199	1019112.488924	40.363636
3180.862485	1021154.816418	40.368653
3183.711457	1023224.061817	40.373671
3186.888732	1025274.317014	40.378688
3190.473423	1027342.691790	40.383706
3193.400017	1029403.841709	40.388724
3196.477107	1031467.971603	40.393741
3199.832699	1033529.361645	40.398759
3202.907400	1035590.903855	40.403776
3206.318720	1037667.829879	40.408794
3209.465004	1039741.710323	40.413812
3212.665320	1041784.354507	40.418829
3215.792075	1043822.020483	40.423847
3219.154513	1045836.557154	40.428864
3222.346157	1047862.519121	40.433882
3225.665435	1049882.522159	40.438900
3229.102725	1051892.917928	40.443917
3232.247394	1053901.284143	40.448935
3235.240824	1055913.558642	40.453952
3238.802453	1057929.521608	40.458970
3241.566190	1059946.799447	40.463988
3244.989195	1061976.384237	40.469005
3247.808604	1064021.636767	40.474023
3251.071141	1066067.302269	40.479040
3255.184894	1068084.729779	40.484058
3258.283010	1070134.564230	40.489076
3261.667409	1072175.917124	40.494093
3264.623182	1074221.177830	40.499111
3267.447914	1076282.359025	40.504128
3271.002435	1078334.217616	40.509146
3273.918569	1080416.511493	40.514164
3276.906403	1082500.102704	40.519181
3279.948076	1084600.004571	40.524199
3282.680926	1086697.808554	40.529216
3285.956599	1088815.543325	40.534234
3288.811822	1090955.635282	40.539252
3292.056457	1093085.844098	40.544269
3295.164862	1095240.146844	40.549287
3297.619352	1097399.996172	40.554304
3301.280090	1099573.755702	40.559322
3304.046211	1101758.321628	40.564340
3307.263986	1103945.644778	40.569357
3310.744036	1106149.942967	40.574375
3313.846176	1108361.588556	40.579392
3317.738615	1110564.200644	40.584410
3320.868129	1112783.919127	40.589428
3324.257006	1115015.608691	40.594445
3327.606651	1117240.102606	40.599463
3330.803506	1119479.849002	40.604480
3334.282527	1121711.393655	40.609498
3337.368271	1123957.829250	40.614516
3340.967442	1126194.125661	40.619533
3344.148715	1128442.831728	40.624551
3347.449423	1130706.970551	40.629568
3350.575861	1132975.197249	40.634586
3353.746018	1135247.753422	40.639604
3356.770325	1137522.390766	40.644621
3360.251786	1139809.984685	40.649639
3363.261427	1142097.708995	40.654656
3366.508842	1144390.457080	40.659674
3369.769834	1146699.316837	40.664692
3373.025214	1149010.002149	40.669709
3376.236902	1151328.370531	40.674727
3379.219447	1153637.071634	40.679744
3382.628890	1155959.691994	40.684762
3385.971690	1158313.363564	40.689780
3388.933973	1160647.376643	40.694797
3392.183823	1162996.793581	40.699815
3395.493572	1165354.753756	40.704832
3399.117482	1167714.611901	40.709850
3402.175188	1170084.695518	40.714868
3405.520090	1172438.511948	40.719885
3409.136731	1174811.904386	40.724903
3412.029677	1177204.820264	40.729920
3415.548382	1179589.017634	40.734938
3418.782378	1181974.608536	40.739956
3422.410330	1184368.140438	40.744973
3426.055860	1186757.093184	40.749991
3429.184989	1189155.341507	40.755008
3432.989495	1191519.405157	40.760013
3436.205102	1193848.400583	40.765018
3439.447183	1196101.150394	40.770023
3443.037237	1198302.658881	40.775028
3446.586510	1200398.373916	40.780032
3450.043227	1202415.714847	40.785037
3453.147737	1204371.966288	40.790042
3456.255704	1206234.161445	40.795047
3459.385781	1208023.096059	40.800052
3462.050263	1209727.410985	40.805056
3464.934254	1211343.240037	40.810061
3467.749501	1212891.952862	40.815066
3469.929135	1214349.945076	40.820071
3472.503702	1215733.956375	40.825076
3474.407765	1217047.026619	40.830080
3476.895545	1218278.442328	40.835085
3479.041529	1219462.895324	40.840090
3481.228802	1220566.536226	40.845095
3483.482718	1221602.956769	40.850100
3485.146634	1222580.804119	40.855104
3486.936294	1223492.151144	40.860109
3488.544328	1224349.966867	40.865114
3490.440319	1225143.467086	40.870119
3492.731473	1225863.984976	40.875124
3494.117361	1226542.932257	40.880128
3495.592383	1227168.965738	40.885133
3497.037030	1227749.774485	40.890138
3498.463201	1228287.610793	40.895143
3500.124283	1228763.325899	40.900148
3501.372891	1229214.629240	40.905152
3502.751854	1229590.147070	40.910157
3503.633189	1229951.824756	40.915162
3504.855161	1230256.728256	40.920167
3505.808606	1230543.848968	40.925172
3506.823896	1230778.825256	40.930176
3507.456576	1230985.977672	40.935181
3508.515566	1231180.931859	40.940186
3509.549367	1231327.033211	40.945191
3510.320459	1231442.596720	40.950196
3510.660542	1231543.126846	40.955200
3511.254906	1231613.037247	40.960205
3512.043082	1231667.720197	40.965210
3512.517382	1231688.895899	40.970215
3513.668856	1231686.841987	40.975220
3513.754562	1231677.785801	40.980224
3514.615977	1231625.441592	40.985229
3515.045404	1231568.040881	40.990234
3515.205565	1231496.887107	40.995239
3515.859035	1231404.303031	41.000244
3515.831601	1231304.930757	41.005248
3516.331724	1231185.239387	41.010253
3516.819432	1231056.224285	41.015258
3516.817617	1230909.199486	41.020263
3517.898122	1230747.727200	41.025268
3517.668536	1230583.948094	41.030272
3518.195981	1230393.744904	41.035277
3518.364600	1230207.043742	41.040282
3518.417036	1230001.705067	41.045287
3519.014682	1229790.859614	41.050292
3518.955250	1229579.647319	41.055296
3519.142059	1229332.013879	41.060301
3519.634738	1229102.877839	41.065306
3519.729136	1228859.806552	41.070311
3520.019513	1228595.611252	41.075316
3519.895202	1228341.358119	41.080320
3520.430686	1228077.468569	41.085325
3520.628518	1227801.026830	41.090330
3520.782813	1227513.661712	41.095335
3520.940955	1227209.672236	41.100340
3520.527920	1226933.843623	41.105344
3520.821458	1226625.598095	41.110349
3520.959721	1226336.022735	41.115354
3520.805263	1226037.800124	41.120359
3521.316495	1225728.531033	41.125364
3520.869475	1225411.934245	41.130368
3521.111630	1225090.257219	41.135373
3521.082408	1224782.232896	41.140378
3521.360938	1224465.644285	41.145383
3521.613244	1224134.476601	41.150388
3521.322492	1223817.007743	41.155392
3521.798903	1223486.881290	41.160397
3522.038226	1223148.555444	41.165402
3521.925639	1222811.105462	41.170407
3521.937950	1222465.674564	41.175412
3521.652011	1222132.410507	41.180416
3522.140911	1221774.526177	41.185421
3521.975476	1221438.955213	41.190426
3522.391598	1221082.061622	41.195431
3522.500735	1220728.650078	41.200436
3522.269432	1220352.193784	41.205440
3522.217808	1220008.101299	41.210445
3522.427380	1219638.620492	41.215450
3522.189906	1219285.259229	41.220455
3522.420647	1218916.750457	41.225460
3522.003406	1218562.247184	41.230464
3522.171274	1218187.901553	41.235469
3521.971478	1217839.948281	41.240474
3521.999009	1217472.770596	41.245479
3522.218205	1217093.942617	41.250484
3522.411844	1216722.102675	41.255488
3522.456738	1216339.414121	41.260493
3522.129864	1215968.726959	41.265498
3521.802079	1215611.198398	41.270503
3521.917031	1215226.076921	41.275508
3521.985381	1214859.545988	41.280512
3522.400237	1214483.297665	41.285517
3522.162919	1214120.224734	41.290522
3521.913620	1213754.040882	41.295527
3522.256215	1213378.003646	41.300532
3521.873435	1213003.368043	41.305536
3521.981198	1212630.776229	41.310541
3522.042301	1212261.159319	41.315546
3521.948427	1211892.102684	41.320551
3522.247462	1211512.379201	41.325556
3522.030479	1211131.589352	41.330560
3522.252332	1210751.354080	41.335565
3522.294889	1210383.663705	41.340570
3521.944051	1209993.356594	41.345575
3522.252750	1209606.187894	41.350580
3521.627358	1209240.585061	41.355584
3521.950619	1208858.507043	41.360589
3521.752685	1208474.707107	41.365594
3521.631714	1208089.460950	41.370599
3521.656446	1207720.645617	41.375604
3521.411686	1207355.126364	41.380608
3521.562222	1206969.095553	41.385613
3521.565266	1206595.519194	41.390618
3521.619556	1206210.383859	41.395623
3521.977121	1205845.032410	41.400628
3521.662647	1205473.581479	41.405632
3521.591209	1205094.098611	41.410637
3521.636359	1204704.166326	41.415642
3521.676565	1204329.575286	41.420647
3522.020985	1203946.190205	41.425652
3521.788348	1203562.309116	41.430656
3521.535988	1203178.215071	41.435661
3521.694298	1202788.587266	41.440666
3521.511517	1202417.830806	41.445671
3521.935981	1202024.069705	41.450676
3521.785070	1201655.409475	41.455680
3521.264274	1201251.430253	41.460685
3521.466606	1200877.873465	41.465690
3521.321812	1200502.564690	41.470695
3521.665195	1200114.204168	41.475700
3521.628176	1199733.944089	41.480704
3521.659260	1199353.550860	41.485709
3521.555515	1198962.831752	41.490714
3521.384737	1198579.130866	41.495719
3521.485339	1198191.228065	41.500724
3521.075255	1197814.828466	41.505728
3521.198482	1197424.705869	41.510733
3521.043744	1197048.114295	41.515738
3520.736942	1196681.750897	41.520743
3521.166445	1196298.344248	41.525748
3520.804327	1195924.520639	41.530752
3520.867819	1195550.318161	41.535757
3520.547199	1195176.433427	41.540762
3520.488444	1194812.431149	41.545767
3520.802217	1194423.458232	41.550772
3520.697582	1194053.400278	41.555776
3520.653173	1193676.168374	41.560781
3520.498825	1193312.733352	41.565786
3520.654219	1192938.326122	41.570791
3520.584101	1192562.425914	41.575796
3520.204553	1192198.667688	41.580800
3520.498651	1191818.895695	41.585805
3520.604421	1191452.938131	41.590810
3520.263136	1191083.551687	41.595815
3520.446412	1190714.334327	41.600820
3520.088782	1190354.013279	41.605824
3519.905860	1189977.285571	41.610829
3519.697872	1189610.403280	41.615834
3519.863061	1189254.524856	41.620839
3520.310918	1188884.193196	41.625844
3519.891820	1188527.702954	41.630848
3520.208405	1188161.947571	41.635853
3520.068871	1187792.762663	41.640858
3519.914749	1187427.691029	41.645863
3520.491115	1187064.165946	41.650868
3520.067650	1186694.667328	41.655872
3519.837644	1186319.279490	41.660877
3519.890082	1185955.292576	41.665882
3519.905394	1185591.944616	41.670887
3519.674924	1185222.497229	41.675892
3519.486721	1184855.744685	41.680896
3519.352203	1184483.876941	41.685901
3519.808644	1184133.901734	41.690906
3519.587917	1183781.756166	41.695911
3519.591895	1183409.412130	41.700916
3519.717194	1183055.089987	41.705920
3519.715203	1182687.212213	41.710925
3519.580861	1182333.071724	41.715930
3519.422449	1181964.697855	41.720935
3519.212484	1181608.355414	41.725940
3519.308836	1181254.385685	41.730944
3519.290333	1180899.751705	41.735949
3519.047687	1180537.315723	41.740954
3519.009121	1180198.360637	41.745959
3519.136706	1179835.343879	41.750964
3518.926392	1179475.935938	41.755968
3519.016514	1179122.575254	41.760973
3519.018240	1178764.119103	41.765978
3518.969426	1178423.354528	41.770983
3518.874304	1178069.010789	41.775988
3518.536310	1177714.965501	41.780992
3518.784648	1177364.285318	41.785997
3518.695837	1177021.645433	41.791002
3518.391144	1176679.301192	41.796007
3518.967129	1176315.022421	41.801012
3518.744706	1175972.335413	41.806016
3518.819963	1175618.927466	41.811021
3518.659546	1175275.524659	41.816026
3518.690684	1174912.745441	41.821031
3518.919658	1174566.215556	41.826036
3518.658546	1174222.288543	41.831040
3518.741348	1173879.696275	41.836045
3518.527076	1173527.608138	41.841050
3518.733155	1173176.841266	41.846055
3518.545166	1172814.046218	41.851060
3518.284922	1172467.174378	41.856064
3518.440269	1172127.849732	41.861069
3518.209412	1171777.343542	41.866074
3517.917501	1171436.255621	41.871079
3518.150711	1171092.795128	41.876084
3517.887129	1170765.052621	41.881088
3518.197847	1170427.478340	41.886093
3518.057228	1170077.314701	41.891098
3517.900594	1169740.622037	41.896103
3518.268180	1169401.934225	41.901108
3517.868919	1169059.293230	41.906112
3517.825264	1168716.288074	41.911117
3517.767941	1168395.629014	41.916122
3517.775556	1168051.816790	41.921127
3518.174339	1167712.636768	41.926132
3517.693116	1167377.732872	41.931136
3517.736638	1167054.426313	41.936141
3517.920048	1166699.734904	41.941146
3517.503420	1166356.919455	41.946151
3517.837265	1166011.125449	41.951156
3517.461585	1165689.030883	41.956160
3517.537943	1165355.227443	41.961165
3517.823606	1165011.452690	41.966170
3517.306353	1164681.103611	41.971175
3517.524381	1164349.195884	41.976180
3517.687542	1164031.727245	41.981184
3517.541363	1163688.692328	41.986189
3517.619782	1163350.132205	41.991194
3517.430710	1163031.527355	41.996199
3517.426959	1162687.931060	42.001204
3517.320239	1162352.171177	42.006208
3517.417399	1162014.655412	42.011213
3517.304715	1161688.586222	42.016218
3517.189521	1161361.741157	42.021223
3517.336250	1161029.918278	42.026228
3517.097810	1160713.826736	42.031232
3517.079920	1160381.517371	42.036237
3517.101144	1160050.787399	42.041242
3516.876527	1159727.166746	42.046247
3517.040899	1159396.088327	42.051252
3517.173491	1159072.273907	42.056256
3517.059314	1158747.818318	42.061261
3516.798002	1158417.977397	42.066266
3516.598914	1158080.540796	42.071271
3516.917010	1157762.855908	42.076276
3516.713346	1157450.344524	42.081280
3516.720083	1157137.969037	42.086285
3517.000461	1156812.666819	42.091290
3516.722820	1156486.963425	42.096295
3516.607662	1156163.672499	42.101300
3516.374624	1155848.895007	42.106304
3516.249282	1155533.513292	42.111309
3516.193186	1155219.520400	42.116314
3516.060717	1154907.413649	42.121319
3516.149016	1154583.329682	42.126324
3516.048528	1154286.225627	42.131328
3516.105147	1153973.180637	42.136333
3516.262731	1153656.314854	42.141338
3515.952849	1153359.192919	42.146343
3515.893504	1153041.947286	42.151348
3516.033726	1152740.267743	42.156352
3516.146763	1152422.861750	42.161357
3516.262421	1152110.642834	42.166362
3516.078716	1151813.696851	42.171367
3515.916754	1151492.966582	42.176372
3515.503498	1151189.585141	42.181376
3515.787469	1150883.041367	42.186381
3515.663329	1150569.444933	42.191386
3515.678567	1150268.401904	42.196391
3515.855485	1149958.223386	42.201396
3515.609376	1149660.976897	42.206400
3515.500382	1149349.294269	42.211405
3515.306034	1149054.088777	42.216410
3515.390753	1148760.620596	42.221415
3515.505874	1148465.899567	42.226420
3515.876883	1148160.604109	42.231424
3515.568452	1147852.465863	42.236429
3515.396663	1147551.866967	42.241434
3515.019602	1147253.843096	42.246439
3515.330082	1146965.354548	42.251444
3515.061558	1146666.426798	42.256448
3515.158835	1146365.052635	42.261453
3515.192724	1146078.930441	42.266458
3515.139661	1145784.561222	42.271463
3514.627183	1145475.843896	42.276468
3514.805571	1145196.474637	42.281472
3514.837971	1144899.198285	42.286477
3514.837586	1144619.543578	42.291482
3514.919863	1144324.217481	42.296487
3514.988667	1144029.351158	42.301492
3514.971995	1143749.842738	42.306496
3514.756726	1143455.275627	42.311501
3514.835863	1143166.997015	42.316506
3514.690331	1142880.920825	42.321511
3514.931366	1142594.291309	42.326516
3514.778066	1142313.117213	42.331520
3514.596350	1142018.085146	42.336525
3514.525620	1141716.473506	42.341530
3514.482624	1141440.546622	42.346535
3514.696610	1141162.191462	42.351540
3514.307695	1140884.110696	42.356544
3514.739795	1140589.277349	42.361549
3514.752068	1140304.838460	42.366554
3514.235320	1140029.105784	42.371559
3514.623927	1139743.910606	42.376564
3514.478660	1139456.130993	42.381568
3514.462505	1139171.920622	42.386573
3514.679846	1138904.834056	42.391578
3514.300964	1138621.697845	42.396583
3514.260431	1138323.399537	42.401588
3513.910043	1138039.942806	42.406592
3514.245933	1137768.223345	42.411597
3514.339182	1137504.029264	42.416602
3514.041278	1137218.241673	42.421607
3514.109744	1136936.650570	42.426612
3513.748014	1136669.072041	42.431616
3513.840192	1136389.821584	42.436621
3514.262258	1136119.997414	42.441626
3513.712145	1135846.426368	42.446631
3513.872351	1135570.730005	42.451636
3514.042267	1135302.235274	42.456640
3513.998139	1135017.236981	42.461645
3514.087651	1134744.643466	42.466650
3513.852914	1134482.537427	42.471655
3514.211360	1134214.906491	42.476660
3514.057850	1133929.487883	42.481664
3513.677100	1133644.946337	42.486669
3513.779095	1133377.315444	42.491674
3513.571801	1133120.077750	42.496679
3513.722529	1132830.939757	42.501684
3513.749695	1132574.967230	42.506688
3513.591063	1132292.407024	42.511693
3513.793279	1132032.863768	42.516698
3513.651062	1131759.775155	42.521703
3513.427740	1131492.483059	42.526708
3513.505523	1131225.888260	42.531712
3513.676519	1130953.466981	42.536717
3513.752444	1130689.031631	42.541722
3513.288425	1130417.828109	42.546727
3513.705430	1130154.355619	42.551732
3513.048517	1129891.522281	42.556736
3513.078684	1129623.809340	42.561741
3513.194752	1129361.678148	42.566746
3512.898036	1129109.109879	42.571751
3513.348640	1128848.039247	42.576756
3513.268091	1128596.647149	42.581760
3513.058653	1128322.061911	42.586765
3512.963303	1128055.812283	42.591770
3512.863716	1127820.838485	42.596775
3513.206407	1127549.926566	42.601780
3513.089184	1127286.400170	42.606784
3513.145153	1127035.197230	42.611789
3513.220606	1126779.984208	42.616794
3512.932553	1126516.257624	42.621799
3512.859560	1126252.767960	42.626804
3513.045947	1125996.928406	42.631808
3513.214978	1125743.838455	42.636813
3513.054734	1125493.169299	42.641818
3512.990861	1125230.579055	42.646823
3512.708498	1124970.010065	42.651828
3512.383800	1124722.566949	42.656832
3512.229013	1124477.368235	42.661837
3512.627486	1124218.743965	42.666842
3512.148802	1123968.150754	42.671847
3512.435577	1123725.699886	42.676852
3512.545791	1123486.503165	42.681856
3512.747929	1123238.523753	42.686861
3512.510657	1122985.845819	42.691866
3512.220392	1122737.257913	42.696871
3512.292568	1122491.264240	42.701876
3512.145390	1122239.773718	42.706880
3512.115196	1121998.439054	42.711885
3512.054139	1121757.098572	42.716890
3511.801716	1121534.250150	42.721895
3512.116076	1121281.400728	42.726900
3511.697215	1121051.703896	42.731904
3511.793274	1120808.771157	42.736909
3512.076529	1120576.557611	42.741914
3511.778025	1120339.477592	42.746919
3511.988878	1120092.684025	42.751924
3511.760108	1119863.761987	42.756928
3511.769077	1119628.504668	42.761933
3511.899026	1119394.074343	42.766938
3511.464631	1119170.585836	42.771943
3511.798853	1118928.195239	42.776948
3511.728301	1118696.339381	42.781952
3511.408364	1118456.416753	42.786957
3511.894187	1118233.213875	42.791962
3511.348728	1117996.165921	42.796967
3511.629867	1117761.925027	42.801972
3511.438864	1117544.140609	42.806977
3511.368821	1117314.130482	42.811981
3511.500188	1117068.068108	42.816986
3511.278183	1116852.452400	42.821991
3511.362580	1116614.763051	42.826996
3511.377116	1116399.852574	42.832001
3511.103361	1116161.916205	42.837005
3511.385639	1115943.607514	42.842010
3510.929484	1115726.936618	42.847015
3511.182893	1115493.172986	42.852020
3511.144429	1115284.327038	42.857025
3511.212566	1115048.382058	42.862029
3511.210773	1114833.030120	42.867034
3511.192715	1114616.814183	42.872039
3511.231665	1114380.939976	42.877044
3511.060391	1114159.105709	42.882049
3511.138291	1113947.614221	42.887053
3511.087872	1113717.637164	42.892058
3511.023739	1113506.151663	42.897063
3511.111331	1113281.282410	42.902068
3511.182173	1113057.264771	42.907073
3511.037507	1112834.036221	42.912077
3510.947743	1112615.271835	42.917082
3511.211047	1112404.451964	42.922087
3511.026929	1112162.508273	42.927092
3510.983048	1111956.967332	42.932097
3510.899506	1111733.682950	42.937101
3511.197003	1111511.280445	42.942106
3510.870913	1111291.165536	42.947111
3510.908242	1111072.794340	42.952116
3511.030871	1110866.134828	42.957121
3510.911506	1110646.436462	42.962125
3511.077379	1110419.717125	42.967130
3510.515271	1110213.813171	42.972135
3510.587636	1109992.720688	42.977140
3510.609331	1109776.780276	42.982145
3510.377040	1109565.644337	42.987149
3510.529114	1109351.001316	42.992154
3510.457796	1109158.908878	42.997159
3510.168062	1108930.483952	43.002164
3510.269074	1108734.339582	43.007169
3510.242609	1108522.365237	43.012173
3510.192578	1108322.222030	43.017178
3510.274080	1108119.663413	43.022183
3510.233909	1107918.644497	43.027188
3510.164625	1107722.491277	43.032193
3509.897465	1107510.230307	43.037197
3510.382256	1107297.073385	43.042202
3510.112245	1107104.176543	43.047207
3510.125534	1106890.508357	43.052212
3510.058126	1106683.337450	43.057217
3509.885077	1106486.774362	43.062221
3510.209501	1106302.057704	43.067226
3510.086734	1106087.520695	43.072231
3510.415225	1105888.465961	43.077236
3510.261452	1105680.029279	43.082241
3509.823143	1105484.428233	43.087245
3510.119927	1105271.604093	43.092250
3509.891196	1105080.920000	43.097255
3509.747915	1104871.304217	43.102260
3509.910726	1104677.676075	43.107265
3509.680854	1104481.526705	43.112269
3509.960771	1104278.886391	43.117274
3509.499354	1104086.581579	43.122279
3509.692267	1103885.278125	43.127284
3509.801235	1103688.853041	43.132289
3509.753849	1103501.713344	43.137293
3509.923206	1103305.359878	43.142298
3509.511516	1103113.585375	43.147303
3509.630391	1102922.098842	43.152308
3509.498829	1102724.818355	43.157313
3509.390508	1102532.877683	43.162317
3509.623201	1102342.593994	43.167322
3509.350729	1102153.437930	43.172327
3509.748387	1101956.519970	43.177332
3509.513328	1101763.330491	43.182337
3509.492220	1101578.891112	43.187341
3509.784703	1101388.277222	43.192346
3509.482741	1101201.290767	43.197351
3509.400761	1101005.086112	43.202356
3509.081925	1100819.140551	43.207361
3509.092229	1100634.854896	43.212365
3509.106705	1100448.172566	43.217370
3508.941275	1100265.910607	43.222375
3509.224526	1100073.913556	43.227380
3509.296740	1099893.607377	43.232385
3509.374062	1099716.353568	43.237389
3509.241318	1099514.653852	43.242394
3509.264344	1099341.507675	43.247399
3509.418772	1099149.785820	43.252404
3509.260371	1098955.240255	43.257409
3509.477933	1098783.956459	43.262413
3509.390825	1098592.254603	43.267418
3509.052580	1098408.906605	43.272423
3509.253266	1098208.250685	43.277428
3508.916864	1098036.173777	43.282433
3509.042729	1097855.025682	43.287437
3508.756669	1097676.330286	43.292442
3508.795443	1097500.253405	43.297447
3508.788925	1097319.874304	43.302452
3509.011853	1097134.573423	43.307457
3508.584936	1096954.442662	43.312461
3509.086583	1096778.839958	43.317466
3508.540301	1096615.074165	43.322471
3508.859744	1096429.063630	43.327476
3508.899857	1096257.824688	43.332481
3508.568369	1096083.867240	43.337485
3508.882237	1095912.189612	43.342490
3508.652084	1095738.395700	43.347495
3508.738025	1095559.856100	43.352500
3508.657218	1095390.331759	43.357505
3508.293236	1095225.058681	43.362509
3508.646302	1095052.199159	43.367514
3508.416877	1094866.512369	43.372519
3508.377722	1094708.442198	43.377524
3508.295434	1094542.144975	43.382529
3508.244670	1094369.617250	43.387533
3508.305582	1094204.147321	43.392538
3508.379612	1094045.943469	43.397543
3508.174530	1093864.907669	43.402548
3508.559908	1093701.952977	43.407553
3508.519201	1093536.096547	43.412557
3508.324450	1093361.646222	43.417562
3508.403988	1093185.613641	43.422567
3508.506048	1093022.876625	43.427572
3508.734102	1092866.431628	43.432577
3508.416368	1092697.149146	43.437581
3508.062908	1092515.614059	43.442586
3508.159022	1092343.571979	43.447591
3508.282036	1092184.731324	43.452596
3508.607273	1092026.235658	43.457601
3508.365650	1091859.690845	43.462605
3508.511964	1091676.992218	43.467610
3508.171190	1091513.516873	43.472615
3508.200460	1091353.805603	43.477620
3508.299010	1091198.674291	43.482625
3508.120915	1091027.114357	43.487629
3508.415898	1090862.461374	43.492634
3508.180592	1090693.868800	43.497639
3508.361207	1090521.659236	43.502644
3508.400020	1090362.204487	43.507649
3508.347928	1090204.771173	43.512653
3508.231118	1090027.998013	43.517658
3508.239997	1089862.882961	43.522663
3508.340167	1089681.752907	43.527668
3508.255207	1089530.626807	43.532673
3508.045615	1089375.398329	43.537677
3508.460682	1089200.809433	43.542682
3508.092856	1089033.528097	43.547687
3507.944012	1088871.282544	43.552692
3508.291201	1088712.878057	43.557697
3508.142912	1088556.658114	43.562701
3508.140565	1088384.027669	43.567706
3508.110668	1088240.712276	43.572711
3507.729882	1088071.487349	43.577716
3508.073207	1087910.760748	43.582721
3507.995480	1087749.332242	43.587725
3508.337889	1087590.320937	43.592730
3507.928383	1087426.350467	43.597735
3508.032866	1087252.420827	43.602740
3508.003522	1087114.154134	43.607745
3507.628199	1086951.696879	43.612749
3507.952415	1086782.315669	43.617754
3508.059352	1086630.502265	43.622759
3507.836784	1086467.142874	43.627764
3508.095980	1086310.599545	43.632769
3507.762453	1086150.219871	43.637773
3507.642031	1085997.563670	43.642778
3507.544693	1085849.499983	43.647783
3507.399201	1085691.663643	43.652788
3507.584077	1085532.618093	43.657793
3507.629425	1085378.958707	43.662797
3507.785728	1085232.465964	43.667802
3507.520201	1085082.204378	43.672807
3507.558638	1084916.454771	43.677812
3507.803220	1084770.606088	43.682817
3507.616613	1084625.687319	43.687821
3507.559145	1084471.827506	43.692826
3507.423728	1084321.619346	43.697831
3507.793633	1084153.970336	43.702836
3507.960479	1084017.989477	43.707841
3507.329962	1083855.673461	43.712845
3507.636786	1083695.307664	43.717850
3507.457667	1083557.358716	43.722855
3507.305914	1083407.703334	43.727860
3507.267893	1083252.175720	43.732865
3507.147180	1083103.561671	43.737869
3507.326309	1082967.936134	43.742874
3507.265661	1082827.072264	43.747879
3507.451645	1082674.847733	43.752884
3507.514765	1082530.886960	43.757889
3507.195647	1082387.273057	43.762893
3507.588226	1082232.029013	43.767898
3507.287059	1082077.566192	43.772903
3507.269978	1081937.727177	43.777908
3507.186795	1081788.495564	43.782913
3506.810618	1081644.679635	43.787917
3507.014375	1081492.994670	43.792922
3506.191029	1081369.101046	43.797927
3506.729870	1081230.303408	43.802932
3506.800329	1081093.210185	43.807937
3506.615132	1080967.091860	43.812941
3507.245534	1080833.449360	43.817946
3507.057938	1080698.211453	43.822951
3507.267784	1080548.417930	43.827956
3507.418170	1080404.674419	43.832961
3506.981787	1080270.330344	43.837965
3507.021259	1080110.862498	43.842970
3506.804094	1079985.110500	43.847975
3506.770549	1079840.135059	43.852980
3507.158280	1079698.444776	43.857985
3506.767353	1079564.555586	43.862989
3506.746506	1079423.885028	43.867994
3507.169856	1079280.546724	43.872999
3507.065313	1079146.024319	43.878004
3506.916153	1079009.778552	43.883009
3506.625034	1078866.259137	43.888013
3507.243281	1078725.849197	43.893018
3506.549218	1078606.861939	43.898023
3506.600574	1078460.780141	43.903028
3507.058698	1078322.305714	43.908033
3506.600458	1078193.288829	43.913037
3506.913998	1078056.751092	43.918042
3506.612619	1077927.798076	43.923047
3506.543412	1077785.845435	43.928052
3506.758857	1077644.898113	43.933057
3506.839889	1077518.272194	43.938061
3506.486410	1077387.491131	43.943066
3506.474896	1077247.722873	43.948071
3506.535706	1077119.363081	43.953076
3506.798081	1076992.983111	43.958081
3506.370965	1076857.689396	43.963085
3506.546565	1076723.157118	43.968090
3506.742064	1076600.331317	43.973095
3506.445294	1076459.821803	43.978100
3506.332827	1076338.288975	43.983105
3506.313964	1076207.040463	43.988109
3506.456071	1076075.186178	43.993114
3506.196934	1075949.924165	43.998119
3506.216203	1075828.262271	44.003124
3506.447899	1075704.546170	44.008129
3506.241162	1075585.892858	44.013133
3506.614982	1075456.770256	44.018138
3506.559774	1075329.251761	44.023143
3506.356460	1075200.506252	44.028148
3506.444060	1075077.663994	44.033153
3505.866411	1074942.539680	44.038157
3506.286578	1074822.325967	44.043162
3506.580470	1074704.435418	44.048167
3506.308829	1074570.980271	44.053172
3506.186734	1074441.147005	44.058177
3506.368259	1074315.294701	44.063181
3506.462972	1074195.408959	44.068186
3506.209213	1074072.792443	44.073191
3506.233913	1073943.883721	44.078196
3506.300661	1073825.819533	44.083201
3506.027574	1073705.023041	44.088205
3506.261410	1073583.948266	44.093210
3506.206421	1073454.464763	44.098215
3506.188151	1073323.627220	44.103220
3506.611894	1073218.267915	44.108225
3506.092806	1073096.441745	44.113229
3506.228534	1072958.556977	44.118234
3505.987855	1072846.863080	44.123239
3505.866635	1072729.766938	44.128244
3506.218761	1072600.484399	44.133249
3505.870692	1072476.886835	44.138253
3506.447833	1072353.614512	44.143258
3506.023741	1072249.721369	44.148263
3506.084463	1072120.187225	44.153268
3505.934820	1071989.915947	44.158273
3505.983165	1071878.154669	44.163277
3505.887247	1071754.114879	44.168282
3505.840476	1071647.169238	44.173287
3505.842055	1071516.669597	44.178292
3506.115716	1071402.939549	44.183297
3505.989202	1071293.213228	44.188301
3505.942198	1071164.058610	44.193306
3506.071203	1071054.669841	44.198311
3506.230942	1070932.395341	44.203316
3506.070709	1070815.552989	44.208321
3505.927748	1070703.607023	44.213325
3505.978705	1070573.172875	44.218330
3505.803625	1070459.208798	44.223335
3505.883288	1070349.045131	44.228340
3506.255831	1070232.967666	44.233345
3505.864961	1070103.267941	44.238349
3505.827285	1069980.908594	44.243354
3505.822930	1069872.479430	44.248359
3505.676183	1069750.901923	44.253364
3506.051807	1069638.656521	44.258369
3505.851143	1069519.966697	44.263373
3505.848521	1069411.528127	44.268378
3505.755593	1069307.812984	44.273383
3505.805419	1069186.286710	44.278388
3505.934662	1069058.880060	44.283393
3505.600751	1068966.158212	44.288397
3506.002017	1068843.508888	44.293402
3505.713328	1068720.201282	44.298407
3505.633878	1068611.759541	44.303412
3505.845188	1068500.287090	44.308417
3505.407325	1068390.457737	44.313421
3505.375821	1068274.116884	44.318426
3505.622863	1068169.651126	44.323431
3505.363618	1068073.344073	44.328436
3505.773708	1067960.866336	44.333441
3505.806885	1067846.909776	44.338445
3506.107980	1067732.810557	44.343450
3505.776827	1067620.544091	44.348455
3505.774382	1067492.545737	44.353460
3505.776333	1067381.758217	44.358465
3505.352681	1067282.771578	44.363469
3505.673564	1067171.061724	44.368474
3505.225259	1067068.228303	44.373479
3505.284019	1066947.227985	44.378484
3505.413243	1066848.623340	44.383489
3505.297596	1066752.846518	44.388493
3505.380356	1066634.720802	44.393498
3505.329196	1066531.811911	44.398503
3505.396685	1066425.707371	44.403508
3505.788067	1066323.587375	44.408513
3505.589089	1066220.985569	44.413517
3505.292951	1066102.429846	44.418522
3505.381825	1065997.275431	44.423527
3505.438783	1065889.142163	44.428532
3505.753168	1065790.872809	44.433537
3505.295159	1065678.876079	44.438541
3505.240269	1065563.635992	44.443546
3505.590813	1065477.284150	44.448551
3505.433542	1065369.368336	44.453556
3505.450579	1065257.958216	44.458561
3505.288120	1065147.441285	44.463565
3505.286836	1065047.767481	44.468570
3505.478167	1064948.252571	44.473575
3505.290396	1064836.194133	44.478580
3505.685341	1064724.422303	44.483585
3505.401621	1064633.158369	44.488589
3505.588502	1064529.595424	44.493594
3505.599884	1064427.406543	44.498599
3505.131502	1064305.953712	44.503604
3505.258514	1064195.658621	44.508609
3504.974817	1064097.168794	44.513613
3504.902251	1063983.534333	44.518618
3505.081493	1063887.947639	44.523623
3505.090164	1063790.847641	44.528628
3505.172188	1063681.030798	44.533633
3505.142120	1063599.138954	44.538637
3505.574351	1063497.248407	44.543642
3505.396734	1063408.063883	44.548647
3505.009542	1063296.680557	44.553652
3505.068480	1063183.585346	44.558657
3504.911953	1063099.397025	44.563661
3504.992845	1062986.390387	44.568666
3505.132222	1062884.825468	44.573671
3504.913111	1062792.461558	44.578676
3504.982941	1062693.599585	44.583681
3504.819325	1062604.784727	44.588685
3504.784799	1062500.546234	44.593690
3504.559675	1062408.465628	44.598695
3504.650970	1062322.203174	44.603700
3505.055877	1062226.069123	44.608705
3504.754148	1062133.322700	44.613709
3504.608560	1062035.832054	44.618714
3504.916534	1061941.056685	44.623719
3504.754212	1061866.958339	44.628724
3504.947947	1061758.239892	44.633729
3504.750298	1061677.502247	44.638733
3504.672080	1061578.644613	44.643738
3504.818761	1061497.077430	44.648743
3504.939617	1061400.686923	44.653748
3505.072169	1061300.634277	44.658753
3504.546571	1061209.642126	44.663757
3504.840448	1061115.625093	44.668762
3504.622779	1061026.312235	44.673767
3504.468205	1060925.433519	44.678772
3504.922083	1060826.378447	44.683777
3504.552905	1060751.143710	44.688781
3504.526892	1060652.645982	44.693786
3504.307861	1060573.243681	44.698791
3504.122594	1060489.116406	44.703796
3504.398970	1060412.133757	44.708801
3504.286490	1060326.932796	44.713805
3504.559709	1060231.844839	44.718810
3504.607665	1060136.696043	44.723815
3504.428756	1060060.264948	44.728820
3504.483270	1059975.127335	44.733825
3504.589082	1059882.564723	44.738829
3504.343496	1059793.043836	44.743834
3504.435619	1059719.259859	44.748839
3504.682046	1059635.337346	44.753844
3504.846293	1059537.944008	44.758849
3504.468087	1059450.558164	44.763853
3504.378318	1059366.590618	44.768858
3504.604680	1059277.754106	44.773863
3504.253922	1059182.461862	44.778868
3504.601124	1059107.375594	44.783873
3504.328823	1059029.886101	44.788877
3504.471867	1058927.669626	44.793882
3504.540676	1058852.914698	44.798887
3504.391595	1058759.411990	44.803892
3504.609496	1058669.989143	44.808897
3504.138121	1058599.846928	44.813901
3504.041026	1058512.592539	44.818906
3504.301178	1058425.855893	44.823911
3504.312739	1058346.287152	44.828916
3504.185790	1058267.318055	44.833921
3504.172297	1058182.549249	44.838925
3504.598866	1058109.170280	44.843930
3504.582251	1058014.091776	44.848935
3504.365691	1057929.641528	44.853940
3504.392469	1057847.943693	44.858945
3504.232774	1057775.427539	44.863949
3504.404232	1057674.628217	44.868954
3504.522342	1057595.801814	44.873959
3504.162880	1057525.145760	44.878964
3504.503336	1057433.466777	44.883969
3503.978435	1057353.201292	44.888973
3504.181527	1057269.538922	44.893978
3504.490528	1057185.954189	44.898983
3504.408348	1057102.914369	44.903988
3504.351117	1057018.038503	44.908993
3504.105456	1056944.658406	44.913997
3504.301965	1056869.662833	44.919002
3504.367709	1056784.184986	44.924007
3504.216819	1056694.405405	44.929012
3504.205554	1056617.706190	44.934017
3503.862625	1056551.756510	44.939021
3504.054940	1056463.169317	44.944026
3504.441067	1056385.341442	44.949031
3504.208331	1056305.783475	44.954036
3504.249136	1056228.010256	44.959041
3503.995411	1056152.789993	44.964045
3504.102919	1056057.657294	44.969050
3504.004104	1055975.952398	44.974055
3503.896905	1055917.087680	44.979060
3503.858471	1055827.275455	44.984065
3504.124728	1055760.059493	44.989069
3504.163803	1055679.676732	44.994074
3504.175254	1055615.970491	44.999079
3503.987703	1055533.020754	45.004084
3503.857741	1055457.963381	45.009089
3504.010981	1055384.111289	45.014093
3504.122863	1055307.855477	45.019098
3504.071730	1055233.360355	45.024103
3503.670000	1055156.126823	45.029108
3504.001456	1055069.903953	45.034113
3504.143496	1055008.771613	45.039117
3504.169844	1054928.380001	45.044122
3504.102285	1054846.074889	45.049127
3503.845672	1054758.883728	45.054132
3503.858862	1054691.889223	45.059137
3504.109105	1054633.241108	45.064141
3504.322707	1054550.981681	45.069146
3504.347282	1054462.486389	45.074151
3504.179741	1054386.167467	45.079156
3504.106171	1054311.663597	45.084161
3503.890767	1054245.086914	45.089165
3503.960397	1054151.759200	45.094170
3504.146523	1054089.548999	45.099175
3504.088409	1054005.687347	45.104180
3504.239860	1053930.948467	45.109185
3503.960635	1053850.880707	45.114189
3503.916234	1053775.015086	45.119194
3503.863561	1053704.163097	45.124199
3503.758971	1053643.634719	45.129204
3503.814328	1053564.086157	45.134209
3503.766305	1053507.114217	45.139213
3503.927829	1053423.978860	45.144218
3503.623472	1053344.389962	45.149223
3503.573099	1053281.823950	45.154228
3503.819430	1053214.387446	45.159233
3503.632942	1053148.467698	45.164237
3503.727893	1053065.820012	45.169242
3503.919343	1052998.486333	45.174247
3503.418345	1052942.836664	45.179252
3503.763283	1052861.687520	45.184257
3503.807559	1052792.061377	45.189261
3503.740305	1052715.509983	45.194266
3504.001542	1052656.549791	45.199271
3503.735166	1052583.500772	45.204276
3503.838017	1052502.289795	45.209281
3503.603153	1052450.159260	45.214285
3503.817684	1052377.606902	45.219290
3503.763589	1052313.487605	45.224295
3503.718116	1052234.997281	45.229300
3503.830350	1052168.341583	45.234305
3503.532068	1052092.301785	45.239309
3503.346118	1052029.165283	45.244314
3503.663749	1051965.848679	45.249319
3503.106543	1051897.274724	45.254324
3503.404419	1051827.594658	45.259329
3503.173379	1051777.193104	45.264333
3503.412451	1051713.886554	45.269338
3503.477851	1051656.394619	45.274343
3503.112850	1051592.511051	45.279348
3503.450865	1051526.099761	45.284353
3503.564200	1051470.526953	45.289357
3503.404825	1051401.784871	45.294362
3503.375181	1051329.066067	45.299367
3503.111285	1051273.842766	45.304372
3503.393006	1051216.214172	45.309377
3503.297539	1051168.678332	45.314381
3502.982680	1051103.044670	45.319386
3502.984195	1051035.428993	45.324391
3503.178717	1050988.615493	45.329396
3503.424707	1050922.019194	45.334401
3503.114299	1050866.317187	45.339405
3503.404294	1050805.306873	45.344410
3503.233451	1050741.188559	45.349415
3503.128097	1050687.380205	45.354420
3503.166262	1050635.187567	45.359425
3502.818066	1050577.559605	45.364429
3503.154499	1050511.908116	45.369434
3503.366700	1050463.157948	45.374439
3503.327194	1050405.380883	45.379444
3503.356945	1050339.777863	45.384449
3503.197780	1050279.221599	45.389453
3503.139230	1050222.506924	45.394458
3503.330631	1050170.284661	45.399463
3503.168552	1050119.374265	45.404468
3503.372940	1050049.108360	45.409473
3503.068352	1049988.186965	45.414477
3503.192386	1049938.964327	45.419482
3503.279823	1049876.530002	45.424487
3503.064338	1049818.582836	45.429492
3503.565360	1049740.931859	45.434497
3503.487316	1049701.002360	45.439501
3503.379110	1049636.474996	45.444506
3502.947347	1049568.140892	45.449511
3502.924497	1049530.902568	45.454516
3503.123495	1049466.515589	45.459521
3503.112350	1049412.196889	45.464525
3503.472075	1049363.895166	45.469530
3503.526654	1049304.161389	45.474535
3503.087760	1049246.630970	45.479540
3503.550908	1049166.855454	45.484545
3503.093674	1049119.458064	45.489549
3503.369157	1049046.755478	45.494554
3503.317016	1049000.930700	45.499559
3503.434249	1048941.086193	45.504564
3503.023551	1048868.301291	45.509569
3502.907638	1048818.722233	45.514573
3503.474062	1048768.837357	45.519578
3503.299026	1048708.459496	45.524583
3503.249442	1048649.604282	45.529588
3503.130121	1048586.224472	45.534593
3502.977220	1048534.815478	45.539597
3503.142354	1048475.633550	45.544602
3503.375731	1048420.299830	45.549607
3502.772231	1048360.085236	45.554612
3503.297485	1048304.895297	45.559617
3503.061192	1048263.437419	45.564621
3503.135954	1048197.319057	45.569626
3503.323350	1048130.891832	45.574631
3503.429238	1048077.119794	45.579636
3503.555505	1048027.783286	45.584641
3503.288366	1047963.745130	45.589645
3502.894710	1047893.260826	45.594650
3503.347179	1047834.893326	45.599655
3503.337218	1047789.244592	45.604660
3503.262356	1047723.241724	45.609665
3503.436878	1047669.454424	45.614669
3503.166626	1047618.635336	45.619674
3503.494568	1047566.172988	45.624679
3502.878404	1047511.742248	45.629684
3503.044478	1047428.902061	45.634689
3503.156454	1047384.870737	45.639693
3503.044293	1047336.146457	45.644698
3502.829834	1047277.303805	45.649703
3502.751488	1047236.198301	45.654708
3503.218873	1047169.616912	45.659713
3503.280789	1047126.557017	45.664717
3503.107754	1047068.380994	45.669722
3502.918714	1047008.952149	45.674727
3502.897488	1046956.831122	45.679732
3502.954150	1046898.518955	45.684737
3503.170446	1046843.558414	45.689741
3502.982230	1046790.401500	45.694746
3503.121385	1046742.788970	45.699751
3502.605970	1046692.001750	45.704756
3502.729614	1046648.927976	45.709761
3503.307456	1046580.101060	45.714765
3503.242006	1046531.555074	45.719770
3502.875704	1046483.058213	45.724775
3502.641034	1046446.992454	45.729780
3503.009173	1046374.818755	45.734785
3503.036220	1046331.951503	45.739789
3502.812067	1046274.065167	45.744794
3502.879890	1046221.729477	45.749799
3502.652687	1046175.330896	45.754804
3503.041677	1046121.589789	45.759809
3503.228017	1046061.992413	45.764813
3503.040753	1045996.277103	45.769818
3503.281160	1045883.858961	45.774823
3502.865034	1045718.927682	45.779828
3503.189714	1045468.034140	45.784833
3502.831872	1045173.597360	45.789837
3502.670763	1044815.186999	45.794842
3503.124198	1044395.039579	45.799847
3502.548823	1043909.355377	45.804852
3502.701153	1043365.072100	45.809857
3502.423490	1042755.601185	45.814861
3502.479848	1042086.012387	45.819866
3502.547682	1041328.412424	45.824871
3502.462145	1040518.742512	45.829876
3502.167032	1039625.769670	45.834881
3501.995168	1038682.074051	45.839885
3501.601461	1037655.682676	45.844890
3501.731693	1036547.877652	45.849895
3501.204836	1035382.890612	45.854900
3501.136828	1034132.444374	45.859905
3501.086926	1032807.489667	45.864909
3501.102683	1031404.965052	45.869914
3500.987782	1029918.260650	45.874919
3500.530273	1028355.964171	45.879924
3500.077961	1026703.423376	45.884929
3500.077642	1024970.563718	45.889933
3499.539862	1023175.214304	45.894938
3499.394285	1021277.015635	45.899943
3499.048434	1019313.503534	45.904948
3498.953717	1017239.216892	45.909953
3498.564446	1015110.721684	45.914957
3498.167698	1012888.965760	45.919962
3498.168060	1010590.581517	45.924967
3497.480960	1008198.450955	45.929972
3497.456561	1005713.692330	45.934977
3496.944833	1003153.983328	45.939981
3496.421121	1000511.456346	45.944986
3496.343523	997784.071704	45.949991
3495.885346	994977.593473	45.954996
3495.422436	992078.295467	45.960001
3494.831281	989105.954102	45.965005
3494.461480	986026.442356	45.970010
3494.391062	982886.929270	45.975015
3493.667448	979654.848078	45.980020
3493.014730	976331.098764	45.985025
3492.578592	972946.309702	45.990029
3492.099517	969448.161008	45.995034
3491.654978	965892.841481	46.000039
3490.912796	962250.223062	46.005044
3490.374893	958516.826805	46.010049
3489.800300	954703.774684	46.015053
3489.066008	950918.027830	46.020058
3488.508820	947045.085569	46.025063
3487.428216	943091.981764	46.030068
3486.966497	939062.781350	46.035073
3486.578363	934934.579842	46.040077
3485.714926	930733.103326	46.045082
3484.990924	926447.914908	46.050087
3483.812569	922101.553061	46.055092
3483.655457	917663.518591	46.060097
3482.543967	913138.283714	46.065101
3481.574454	908524.522931	46.070106
3481.371314	903842.125782	46.075111
3480.458981	899087.047726	46.080116
3479.512385	894226.833337	46.085121
3478.394849	889299.314662	46.090125
3477.487774	884293.548423	46.095130
3476.887171	879198.989469	46.100135
3475.672044	874031.908914	46.105140
3474.817464	868767.629687	46.110145
3473.799762	863427.517514	46.115149
3473.167591	858007.541998	46.120154
3472.378773	852491.472801	46.125159
3470.674791	846920.758197	46.130164
3469.750570	841241.331406	46.135169
3468.886007	835486.378900	46.140173
3467.869794	829665.718183	46.145178
3466.700464	823753.173117	46.150183
3465.630496	817759.196770	46.155188
3464.502769	811676.858186	46.160193
3463.382393	805523.148092	46.165197
3462.151052	799278.092362	46.170202
3461.132013	792961.123720	46.175207
3459.943546	786549.624274	46.180212
3459.077371	780056.977797	46.185217
3458.008237	773483.388112	46.190221
3456.411584	766825.529022	46.195226
3455.349227	760086.351575	46.200231
3453.690041	753262.168934	46.205236
3452.468108	746363.907272	46.210241
3450.862449	739378.843050	46.215245
3449.714884	732314.539814	46.220250
3448.470105	725161.374576	46.225255
3447.036683	717935.118542	46.230260
3445.632035	710630.944796	46.235265
3444.288314	703246.827815	46.240269
3442.260986	695761.917455	46.245274
3441.206316	688212.746928	46.250279
3439.584890	680597.344750	46.255284
3438.020516	672885.057968	46.260289
3436.867856	665116.993792	46.265293
3435.111313	657240.480504	46.270298
3433.435125	649291.872394	46.275303
3431.670267	641283.425546	46.280308
3430.309312	633193.138116	46.285313
3428.478461	625014.501433	46.290317
3426.730036	616766.528935	46.295322
3424.752501	608441.144686	46.300327
3423.068092	600054.218932	46.305332
3421.552247	591583.943943	46.310337
3420.082978	583044.458068	46.315341
3417.796670	574415.801402	46.320346
3416.039270	565728.608260	46.325351
3413.847768	556973.876276	46.330356
3411.823790	548123.722736	46.335361
3409.655084	539231.323403	46.340365
3407.927150	530261.454158	46.345370
3405.995067	521220.937582	46.350375
3403.813981	512120.361711	46.355380
3402.188904	502935.667070	46.360385
3399.958572	493692.454019	46.365389
3397.385137	484374.639977	46.370394
3395.691903	474996.194899	46.375399
3393.155947	465558.434905	46.380404
3391.483917	456040.573145	46.385409
3389.026868	446469.363176	46.390413
3386.436082	436832.315075	46.395418
3384.202362	427135.225942	46.400423
3381.778482	417370.724969	46.405428
3379.219833	407543.302098	46.410433
3376.710688	397663.665950	46.415437
3374.076254	387737.115853	46.420442
3371.538149	377739.913775	46.425447
3368.446140	367713.094335	46.430452
3365.922254	357625.891479	46.435457
3363.441127	347485.953361	46.440461
3360.834673	337309.663940	46.445466
3357.603946	327076.597269	46.450471
3354.384321	316801.392691	46.455476
3351.621883	306474.038760	46.460481
3348.917634	296138.089415	46.465485
3345.581176	285748.163214	46.470490
3342.245306	275295.733272	46.475495
3338.940187	264832.051595	46.480500
3335.802523	254336.694676	46.485505
3332.270197	243800.971460	46.490509
3328.682468	233250.657792	46.495514
3325.546754	222581.252336	46.500519
3321.526869	211986.322180	46.505524
3317.178311	201357.695202	46.510529
3313.460351	190729.998079	46.515533
3309.200535	180099.939045	46.520538
3305.192255	169457.456182	46.525543
3299.965612	158823.751000	46.530548
3295.624489	148182.276368	46.535553
3290.879044	137584.849399	46.540557
3285.463880	126988.884575	46.545562
3280.305606	116412.204664	46.550567
3274.176375	105878.331176	46.555572
3268.474789	95382.155676	46.560577
3262.358386	84940.489229	46.565581
3255.250789	74563.469567	46.570586
3247.973587	64250.445039	46.575591
3239.240327	54065.024726	46.580596
3227.172035	44062.524456	46.585601
3200.736164	34608.719539	46.590605
3169.878981	25553.416812	46.595610
3138.988283	16973.294119	46.600615
3102.461927	9092.020952	46.605620
3043.329076	2501.279997	46.610625
2857.995131	402.064050	46.615629
2672.231358	412.151715	46.620634
2599.903300	394.424820	46.625639
2623.165654	377.165366	46.630644
2698.079302	366.987573	46.635649
2780.478132	352.327415	46.640653
2842.247410	355.278811	46.645658
2875.039026	351.790389	46.650663
2882.875174	359.880468	46.655668
2875.985469	363.796442	46.660673
2864.018898	343.218040	46.665677
2851.402040	344.672998	46.670682
2842.932826	343.276183	46.675687
2838.091438	345.456514	46.680692
2835.755543	346.928410	46.685697
2835.304136	338.136981	46.690701
2833.938198	340.246720	46.695706
2832.702985	314.623498	46.700711
2830.277411	338.417879	46.705716
2827.491350	342.462807	46.710721
2824.491756	334.185303	46.715725
2821.088574	318.902821	46.720730
2818.262093	323.672840	46.725735
2815.193172	319.997441	46.730740
2812.016515	317.611114	46.735745
2808.782741	324.730936	46.740749
2805.584228	319.742259	46.745754
2802.524284	307.804450	46.750759
2799.299798	321.061642	46.755764
2796.555384	312.195330	46.760769
2793.302066	308.738287	46.765773
2789.655036	318.165684	46.770778
2786.384375	313.728670	46.775783
2783.485732	310.923298	46.780788
2780.062568	303.484211	46.785793
2777.190588	304.086533	46.790797
2773.815687	308.745815	46.795802
2770.070980	299.058451	46.800807
2766.376789	306.758330	46.805812
2763.156680	307.158287	46.810817
2760.373908	296.657248	46.815821
2756.788493	308.295381	46.820826
2753.782515	299.192820	46.825831
2750.392320	288.209559	46.830836
2746.726275	303.336604	46.835841
2743.396200	302.396278	46.840845
2739.812737	302.467636	46.845850
2736.776436	295.087128	46.850855
2732.923910	294.881620	46.855860
2729.903482	290.391841	46.860865
2726.645987	292.544122	46.865869
2723.256160	294.063726	46.870874
2720.213210	294.233822	46.875879
2716.488962	289.051590	46.880884
2712.559356	288.937826	46.885889
2709.362548	283.961355	46.890893
2705.419678	292.807122	46.895898
2702.670722	290.430933	46.900903
2699.477705	287.585836	46.905908
2695.986772	296.839136	46.910913
2692.507449	284.867453	46.915917
2688.612133	294.548023	46.920922
2685.999994	290.959468	46.925927
2682.407172	286.234076	46.930932
2678.717522	291.720933	46.935937
2675.523057	284.052115	46.940941
2671.525589	287.939380	46.945946
2668.023370	273.211050	46.950951
2665.063343	284.041075	46.955956
2661.612027	284.344527	46.960961
2657.838112	280.553404	46.965965
2654.272010	282.540141	46.970970
2651.362148	284.354254	46.975975
2647.626291	279.654242	46.980980
2643.975898	278.258690	46.985985
2640.486463	284.991546	46.990989
2636.907444	285.631376	46.995994
2634.064678	282.448271	47.000999
2630.641452	290.104505	47.006004
2627.511180	289.140757	47.011009
2623.703989	282.700753	47.016013
2619.387598	289.193495	47.021018
2616.113082	284.306143	47.026023
2612.949055	277.843068	47.031028
2609.580330	285.150740	47.036033
2606.194699	282.729117	47.041037
2602.775470	277.222190	47.046042
2599.691568	266.372225	47.051047
2595.573572	279.660254	47.056052
2592.240681	291.354660	47.061057
2589.218367	267.879288	47.066061
2585.084028	266.544228	47.071066
2581.542309	267.052045	47.076071
2578.086488	279.795518	47.081076
2575.180969	274.196007	47.086081
2571.670979	267.444504	47.091085
2568.135666	273.135429	47.096090
2564.613737	264.808366	47.101095
2560.674401	269.257617	47.106100
2557.369755	275.642155	47.111105
2554.533989	266.408548	47.116109
2550.384383	268.109644	47.121114
2547.131876	267.585481	47.126119
2543.732990	273.150822	47.131124
2539.951070	259.575743	47.136129
2536.664845	267.127721	47.141133
2532.824010	275.187590	47.146138
2530.177175	252.755723	47.151143
2526.337902	261.080719	47.156148
2522.660596	267.593904	47.161153
2519.600643	265.224677	47.166157
2515.718766	263.454973	47.171162
2512.045614	265.283222	47.176167
2508.686097	268.880675	47.181172
2505.473567	261.870117	47.186177
2502.204908	254.001424	47.191181
2498.290175	266.085392	47.196186
2495.365713	257.974761	47.201191
2491.277189	256.280387	47.206196
2487.941327	271.190544	47.211201
2484.544412	259.329819	47.216205
2480.348680	258.522400	47.221210
2476.895604	263.085363	47.226215
2473.632533	249.360450	47.231220
2470.692567	254.541831	47.236225
2467.431449	256.008647	47.241229
2463.548976	253.196361	47.246234
2460.017560	250.440037	47.251239
2456.566750	258.611617	47.256244
2452.909425	255.858891	47.261249
2449.856883	255.229973	47.266253
2446.122745	259.358737	47.271258
2442.742677	258.839279	47.276263
2439.367626	246.922005	47.281268
2435.428410	260.312504	47.286273
2431.772104	248.451383	47.291277
2428.424872	256.331327	47.296282
2425.231278	240.193181	47.301287
2421.781300	252.845151	47.306292
2418.049712	247.306279	47.311297
2414.946101	254.433549	47.316301
2411.035431	252.882736	47.321306
2407.651705	249.703901	47.326311
2404.508850	242.111574	47.331316
2400.630144	252.397521	47.336321
2397.249553	249.612210	47.341325
2393.755708	250.124945	47.346330
2390.084146	243.894765	47.351335
2386.501114	248.289475	47.356340
2382.758127	248.688214	47.361345
2380.091838	241.109847	47.366349
2376.217063	251.543732	47.371354
2372.828221	252.771097	47.376359
2369.190970	237.609658	47.381364
2366.035523	243.345740	47.386369
2362.466515	241.112925	47.391373
2358.605209	248.693896	47.396378
2355.325860	246.217281	47.401383
2351.975069	246.881657	47.406388
2348.249237	239.817723	47.411393
2344.845745	248.132579	47.416397
2341.408749	242.443648	47.421402
2337.888400	238.203731	47.426407
2334.376734	237.750127	47.431412
2330.694294	245.869972	47.436417
2327.215919	234.286010	47.441421
2323.870920	244.259713	47.446426
2320.734314	248.102831	47.451431
2316.992072	240.689217	47.456436
2313.295168	239.664463	47.461441
2310.161385	237.715356	47.466445
2306.045997	237.303522	47.471450
2302.529423	240.167789	47.476455
2299.646707	237.684289	47.481460
2295.800832	235.006747	47.486465
2292.444364	224.102975	47.491469
2289.006046	243.483633	47.496474
2285.392444	234.940116	47.501479
2281.958324	228.890649	47.506484
2278.156020	242.904321	47.511489
2275.010633	235.871175	47.516493
2271.185802	229.835444	47.521498
2267.487253	224.008662	47.526503
2264.435414	240.463049	47.531508
2260.665878	241.626281	47.536513
2257.840308	240.458237	47.541517
2254.015399	237.986215	47.546522
2250.504083	235.006480	47.551527
2247.036035	243.859240	47.556532
2243.665778	227.493846	47.561537
2240.147813	217.077572	47.566541
2236.082226	241.861844	47.571546
2232.609050	232.424549	47.576551
2229.401349	228.064755	47.581556
2226.157245	230.874149	47.586561
2222.680859	228.198649	47.591565
2219.178524	228.848123	47.596570
2215.344638	234.537715	47.601575
2211.911897	233.765610	47.606580
2208.053991	233.755219	47.611585
2204.967828	220.497061	47.616589
2201.533658	218.294476	47.621594
2197.928484	218.715662	47.626599
2194.780682	227.336252	47.631604
2190.891902	218.085929	47.636609
2187.621863	225.441382	47.641613
2183.922075	231.315851	47.646618
2180.590978	225.990161	47.651623
2176.935442	218.948086	47.656628
2173.335834	231.271411	47.661633
2170.040398	220.740038	47.666637
2166.284661	219.850063	47.671642
2163.029189	230.135895	47.676647
2159.663779	222.721293	47.681652
2155.956471	219.996310	47.686657
2152.512573	223.867581	47.691661
2148.828072	228.906386	47.696666
2145.139896	216.610122	47.701671
2142.164122	218.861089	47.706676
2138.510161	226.587302	47.711681
2134.892420	215.457686	47.716685
2131.363808	218.536321	47.721690
2127.617694	218.196566	47.726695
2124.622642	215.544915	47.731700
2121.261832	222.794706	47.736705
2118.046320	215.332812	47.741709
2114.094712	221.209581	47.746714
2110.505838	225.450477	47.751719
2106.792670	219.377485	47.756724
2103.102105	217.503346	47.761729
2099.901521	217.859912	47.766733
2096.656792	217.825286	47.771738
2093.288664	212.059629	47.776743
2089.580334	218.302250	47.781748
2086.009142	225.659075	47.786753
2082.547007	217.634792	47.791757
2078.704237	227.608695	47.796762
2075.355468	221.062731	47.801767
2072.146679	218.241253	47.806772
2068.538385	213.390408	47.811777
2065.067081	216.276216	47.816781
2061.381362	218.904582	47.821786
2058.082438	206.880294	47.826791
2054.911338	214.026201	47.831796
2050.998821	214.847895	47.836801
2047.470546	203.249565	47.841805
2043.576588	216.652245	47.846810
2040.391648	213.775744	47.851815
2037.127071	209.250019	47.856820
2033.586904	207.905953	47.861825
2030.236296	212.775186	47.866829
2026.502426	217.663053	47.871834
2022.994591	209.145170	47.876839
2019.765461	206.383999	47.881844
2015.536425	214.830904	47.886849
2012.576448	205.701251	47.891853
2008.410547	207.934120	47.896858
2005.184200	213.220504	47.901863
2001.978940	210.972462	47.906868
1998.768231	219.125402	47.911873
1995.358504	219.148032	47.916877
1991.644303	216.715311	47.921882
1988.062980	209.577939	47.926887
1984.829939	207.157893	47.931892
1980.804581	215.917301	47.936897
1977.627172	214.052494	47.941901
1973.965067	215.816524	47.946906
1970.419625	210.188804	47.951911
1966.665900	213.568653	47.956916
1963.363566	208.418088	47.961921
1960.361812	207.227436	47.966925
1956.632099	214.269208	47.971930
1953.050980	215.607404	47.976935
1949.570146	204.913780	47.981940
1945.895732	208.149933	47.986945
1942.500492	204.767142	47.991949
1938.981321	206.122452	47.996954
1935.801585	202.852195	48.001959
1932.024231	207.829655	48.006964
1928.270163	204.443620	48.011969
1924.804670	204.400111	48.016973
1921.435360	204.004316	48.021978
1917.985508	199.946465	48.026983
1914.589235	205.551854	48.031988
1911.047702	212.329276	48.036993
1907.347541	193.368746	48.041997
1903.803656	201.255255	48.047002
1900.521228	213.107637	48.052007
1896.768777	199.519293	48.057012
1893.157810	193.696339	48.062017
1890.240852	201.115478	48.067021
1886.828516	199.116332	48.072026
1883.084184	199.052549	48.077031
1879.822007	198.165548	48.082036
1875.531296	206.662156	48.087041
1872.514408	193.791943	48.092045
1868.801001	203.244191	48.097050
1865.525985	200.466988	48.102055
1861.687217	193.598291	48.107060
1858.383434	200.456273	48.112065
1855.378151	202.350740	48.117069
1851.898204	203.626811	48.122074
1848.012577	199.904701	48.127079
1844.094698	206.722932	48.132084
1840.482512	202.920194	48.137089
1837.362659	201.954681	48.142093
1834.101714	205.374143	48.147098
1830.446296	196.207793	48.152103
1827.026333	177.716886	48.157108
1823.444445	196.737424	48.162113
1820.467032	193.059047	48.167117
1816.649763	185.452042	48.172122
1812.913238	199.338086	48.177127
1809.448499	196.440480	48.182132
1805.845790	201.117877	48.187137
1802.512229	189.394745	48.192141
1798.944787	195.129838	48.197146
1795.363438	189.270879	48.202151
1791.842692	194.790007	48.207156
1787.930440	199.429399	48.212161
1785.018207	193.179364	48.217165
1781.388849	202.893723	48.222170
1777.751256	198.341478	48.227175
1774.372598	189.953084	48.232180
1770.901196	198.616640	48.237185
1767.786086	193.910614	48.242189
1763.886402	196.976645	48.247194
1760.186064	188.910669	48.252199
1756.517711	183.912165	48.257204
1753.162675	196.965074	48.262209
1749.904158	199.220717	48.267213
1746.476277	193.997161	48.272218
1742.913497	191.884891	48.277223
1739.722935	198.577338	48.282228
1735.803669	194.556096	48.287233
1732.680938	181.731158	48.292237
1728.842101	201.610013	48.297242
1725.107447	192.694369	48.302247
1721.706124	181.112797	48.307252
1718.117774	200.447078	48.312257
1714.957885	192.377879	48.317261
1711.607901	193.801469	48.322266
1708.022459	192.242176	48.327271
1704.397041	190.656529	48.332276
1700.625924	204.468120	48.337281
1697.461408	191.118036	48.342285
1693.837234	192.300382	48.347290
1690.408053	204.204074	48.352295
1687.210986	194.551672	48.357300
1683.103540	189.508064	48.362305
1679.897230	182.359710	48.367309
1676.296544	193.019135	48.372314
1672.641813	198.274815	48.377319
1669.779846	185.840179	48.382324
1665.214222	188.784208	48.387329
1662.318062	179.604264	48.392333
1658.958847	192.441932	48.397338
1655.376072	199.740457	48.402343
1651.856961	185.024819	48.407348
1648.254125	199.113897	48.412353
1645.274566	199.632291	48.417357
1641.392352	189.327604	48.422362
1637.492026	195.419686	48.427367
1634.267020	190.643761	48.432372
1630.855504	188.543782	48.437377
1627.319050	184.650533	48.442381
1623.634809	185.810466	48.447386
1620.032751	184.216867	48.452391
1617.169003	186.502229	48.457396
1613.027386	194.366440	48.462401
1609.540596	195.476829	48.467405
1606.070417	189.505020	48.472410
1602.998335	196.506785	48.477415
1599.872892	183.727160	48.482420
1595.891862	182.549103	48.487425
1592.294946	182.160838	48.492429
1589.174360	185.506527	48.497434
1585.343170	190.308740	48.502439
1581.845832	176.874064	48.507444
1578.207661	191.049001	48.512449
1574.594947	186.318247	48.517453
1571.234191	192.239135	48.522458
1567.586210	188.297533	48.527463
1564.295151	191.379541	48.532468
1560.532916	184.054944	48.537473
1557.474137	182.183190	48.542477
1553.731068	177.800513	48.547482
1550.504755	191.767401	48.552487
1546.512079	178.307943	48.557492
1543.283144	190.031140	48.562497
1539.913351	178.432934	48.567501
1536.278993	182.495718	48.572506
1532.717180	185.791223	48.577511
1529.283151	185.838705	48.582516
1525.467077	177.345461	48.587521
1522.183636	177.174434	48.592525
1518.441614	182.103533	48.597530
1515.173316	173.671530	48.602535
1511.695606	178.173832	48.607540
1508.248156	187.711668	48.612545
1504.658296	172.588626	48.617549
1501.583091	179.339166	48.622554
1497.426047	185.382227	48.627559
1494.222591	169.534133	48.632564
1490.448928	174.270760	48.637569
1487.661367	188.093629	48.642573
1483.762336	177.705802	48.647578
1480.511234	189.683658	48.652583
1476.822521	184.736620	48.657588
1472.892890	188.224367	48.662593
1469.812649	170.538416	48.667597
1466.021701	174.350740	48.672602
1462.315524	186.237965	48.677607
1459.069247	173.556705	48.682612
1455.845220	177.134885	48.687617
1452.335664	176.734049	48.692621
1448.824032	176.398474	48.697626
1444.848112	184.262055	48.702631
1441.661573	184.040444	48.707636
1438.394878	189.563966	48.712641
1435.036046	177.371686	48.717645
1430.977370	188.888838	48.722650
1427.730690	180.533322	48.727655
1424.144795	187.651127	48.732660
1420.471975	196.823092	48.737665
1417.280530	187.687169	48.742669
1413.653148	183.170742	48.747674
1409.675642	188.161551	48.752679
1407.035556	184.725533	48.757684
1402.855325	189.268662	48.762689
1399.434146	183.242712	48.767693
1396.104209	183.552571	48.772698
1392.765894	182.834342	48.777703
1389.398153	182.367808	48.782708
1385.443304	187.107856	48.787713
1381.984535	176.229723	48.792717
1378.373237	173.390277	48.797722
1375.016834	176.731961	48.802727
1372.191007	176.310063	48.807732
1368.065212	176.719430	48.812737
1364.659455	180.345106	48.817741
1361.257594	177.601621	48.822746
1357.779622	180.334647	48.827751
1354.012571	183.351275	48.832756
1350.699899	188.088440	48.837761
1347.264170	168.843586	48.842765
1343.331741	175.442768	48.847770
1339.699895	169.837669	48.852775
1336.787890	170.767781	48.857780
1333.207765	181.300325	48.862785
1329.683816	176.161425	48.867789
1325.778036	175.415747	48.872794
1322.341086	191.517457	48.877799
1319.113389	179.107868	48.882804
1315.944632	187.237541	48.887809
1312.152359	175.925267	48.892813
1308.316350	182.286972	48.897818
1304.974231	189.997468	48.902823
1301.604847	168.097527	48.907828
1297.967776	175.471751	48.912833
1294.671611	179.303219	48.917837
1290.972791	176.347154	48.922842
1287.267542	183.649770	48.927847
1283.753797	183.735393	48.932852
1280.217487	181.325401	48.937857
1277.146413	177.252036	48.942861
1273.510885	186.580389	48.947866
1270.090579	176.719133	48.952871
1266.751846	167.898851	48.957876
1262.867637	179.286449	48.962881
1259.632823	168.174217	48.967885
1256.320414	166.773227	48.972890
1252.455037	185.710298	48.977895
1249.185790	176.423749	48.982900
1245.557161	170.198716	48.987905
1242.018927	174.821131	48.992909
1238.551976	175.054435	48.997914
1234.611279	178.623451	49.002919
1231.455229	179.170265	49.007924
1227.793164	187.851300	49.012929
1224.581945	175.108160	49.017933
1221.267580	181.435985	49.022938
1217.494225	179.102352	49.027943
1213.873785	175.444777	49.032948
1210.293426	179.414057	49.037953
1206.974059	172.554841	49.042957
1203.462471	167.813431	49.047962
1200.141430	187.422877	49.052967
1196.641111	169.350559	49.057972
1192.732499	178.810839	49.062977
1189.072334	178.328256	49.067981
1186.000631	170.175244	49.072986
1182.227994	181.479151	49.077991
1179.121878	159.343670	49.082996
1175.395859	173.613055	49.088001
1172.120433	173.250466	49.093005
1168.624200	170.096175	49.098010
1164.103320	173.837071	49.103015
1161.321965	163.678031	49.108020
1158.117185	175.334516	49.113025
1155.045176	169.577123	49.118029
1151.413875	172.064650	49.123034
1147.320931	175.677788	49.128039
1144.076291	167.500470	49.133044
1140.094144	168.162691	49.138049
1136.511680	175.466412	49.143053
1133.292363	173.703044	49.148058
1129.695821	174.390105	49.153063
1126.553175	168.773626	49.158068
1122.739706	171.611181	49.163073
1119.158991	165.128719	49.168077
1115.868623	169.342581	49.173082
1112.205417	173.683507	49.178087
1109.089185	164.787813	49.183092
1105.434607	164.550400	49.188097
1102.161185	168.162830	49.193101
1098.473903	173.618694	49.198106
1094.609947	161.856114	49.203111
1091.569087	159.862050	49.208116
1087.782429	162.857089	49.213121
1084.376562	160.234083	49.218125
1080.913753	161.719705	49.223130
1077.151936	169.317358	49.228135
1073.924217	155.451394	49.233140
1070.156733	156.902873	49.238145
1066.802898	152.104327	49.243149
1063.361292	157.200295	49.248154
1059.627117	164.003359	49.253159
1056.301068	157.528417	49.258164
1052.218128	171.080162	49.263169
1049.500107	160.799738	49.268173
1046.194348	160.372075	49.273178
1042.559994	168.514093	49.278183
1038.948369	153.583610	49.283188
1035.087353	158.786623	49.288193
1031.921286	167.473547	49.293197
1028.683719	155.788334	49.298202
1024.736845	153.544435	49.303207
1021.193538	159.856763	49.308212
1017.717803	159.074987	49.313217
1014.299683	163.306139	49.318221
1010.881719	149.312697	49.323226
1007.153047	158.047726	49.328231
1003.895293	160.915528	49.333236
1000.230320	167.163902	49.338241
996.752264	151.630713	49.343245
993.343889	165.660075	49.348250
989.671298	161.435984	49.353255
986.534292	157.216991	49.358260
982.696639	161.376447	49.363265
979.178327	160.987661	49.368269
975.717018	165.313567	49.373274
972.165146	155.706761	49.378279
968.846963	162.059978	49.383284
965.250906	165.121971	49.388289
961.554396	163.303309	49.393293
958.183952	162.350475	49.398298
954.556789	162.806109	49.403303
951.217200	154.199355	49.408308
947.411580	160.321808	49.413313
944.232309	155.945654	49.418317
941.055652	158.463679	49.423322
936.907081	161.849248	49.428327
934.000109	159.635347	49.433332
930.370997	164.998223	49.438337
926.906998	155.803421	49.443341
923.384260	163.719095	49.448346
919.908828	158.235025	49.453351
916.227540	150.053686	49.458356
912.294604	156.598013	49.463361
908.810722	157.418417	49.468365
905.484422	149.670166	49.473370
902.068494	149.439726	49.478375
898.914172	156.539863	49.483380
895.037764	156.905868	49.488385
891.772395	146.238820	49.493389
888.152431	159.298154	49.498394
884.660545	151.119102	49.503399
881.489745	150.721030	49.508404
877.745101	148.179235	49.513409
873.974600	156.338872	49.518413
870.446929	146.579861	49.523418
866.655481	151.371918	49.528423
863.767104	154.383102	49.533428
860.296804	147.801476	49.538433
856.663688	146.104705	49.543437
853.517637	143.506896	49.548442
849.475238	147.755377	49.553447
846.232770	151.777257	49.558452
842.488348	148.107228	49.563457
839.320385	147.290312	49.568461
835.618670	139.524978	49.573466
832.005914	152.077928	49.578471
828.759223	143.471203	49.583476
825.426778	154.070771	49.588481
821.592616	151.654580	49.593485
818.332717	151.466884	49.598490
814.448461	155.649415	49.603495
810.887669	158.857886	49.608500
807.515701	154.376099	49.613505
804.116645	150.085642	49.618509
800.449703	143.748437	49.623514
796.914228	156.076533	49.628519
793.470952	148.766060	49.633524
789.901962	146.734952	49.638529
786.610449	151.824609	49.643533
783.349186	153.081364	49.648538
779.632790	157.142275	49.653543
776.432567	154.418587	49.658548
772.548688	158.144800	49.663553
768.556074	148.701182	49.668557
765.405506	157.582360	49.673562
762.054398	163.917328	49.678567
758.744969	147.494610	49.683572
754.999809	163.658430	49.688577
751.398196	159.906959	49.693581
748.178213	148.250095	49.698586
744.632432	146.319853	49.703591
740.803021	138.896198	49.708596
737.447459	156.060457	49.713601
734.053772	141.197008	49.718605
730.406476	138.292947	49.723610
726.954077	147.745963	49.728615
723.850822	150.115918	49.733620
720.334718	155.649450	49.738625
716.549604	146.757118	49.743629
713.186785	146.729323	49.748634
709.320739	147.864909	49.753639
705.972997	142.697281	49.758644
702.262576	143.398146	49.763649
698.895888	140.500935	49.768653
695.673550	139.655186	49.773658
691.861359	133.920158	49.778663
688.767874	147.623151	49.783668
684.498772	149.182053	49.788673
681.215857	145.682243	49.793677
678.016055	146.487418	49.798682
674.581837	150.817375	49.803687
671.266823	145.207615	49.808692
667.798402	143.474379	49.813697
664.237297	139.792040	49.818701
660.591038	139.766691	49.823706
656.532112	146.100315	49.828711
653.465406	146.644972	49.833716
649.840087	146.038646	49.838721
646.336263	142.276515	49.843725
642.889303	136.853123	49.848730
639.424663	144.523830	49.853735
636.015893	134.547339	49.858740
632.081876	145.158925	49.863745
628.726017	135.441843	49.868749
625.795507	133.622451	49.873754
621.939525	145.378273	49.878759
618.578366	143.506200	49.883764
615.111489	132.197026	49.888769
611.333133	141.225450	49.893773
607.877530	137.755782	49.898778
604.310129	143.861945	49.903783
600.791088	140.803691	49.908788
597.336938	139.297805	49.913793
593.940449	136.821304	49.918797
590.597242	138.560592	49.923802
586.637859	139.758427	49.928807
583.565261	133.771677	49.933812
579.515574	137.477827	49.938817
575.895798	143.309911	49.943821
572.991018	134.965325	49.948826
569.316897	138.028274	49.953831
566.127603	135.159745	49.958836
562.551024	146.363545	49.963841
558.969222	137.688720	49.968845
555.979742	135.752725	49.973850
552.089386	150.453969	49.978855
548.526073	134.776159	49.983860
544.694091	139.211436	49.988865
540.843083	145.342969	49.993869
537.112763	139.984496	49.998874
534.232454	132.260275	50.003879
530.779193	129.005135	50.008884
527.593063	143.578814	50.013889
523.975683	141.324999	50.018893
520.254773	135.565038	50.023898
516.635792	137.249977	50.028903
513.374721	138.149899	50.033908
509.972817	139.790796	50.038913
506.224504	142.660538	50.043917
503.013128	140.540037	50.048922
499.271605	143.768750	50.053927
495.940159	140.382914	50.058932
492.130378	148.681811	50.063937
488.948338	140.818527	50.068941
485.798173	131.392723	50.073946
481.725838	147.697791	50.078951
478.160091	138.223829	50.083956
474.354408	134.653036	50.088961
470.945365	140.416225	50.093965
467.648706	133.229423	50.098970
464.362827	136.570921	50.103975
460.894890	142.113881	50.108980
457.513348	135.617974	50.113985
453.658619	137.974956	50.118989
450.349986	124.590603	50.123994
446.489708	142.326656	50.128999
443.524025	142.687010	50.134004
439.881456	133.021454	50.139009
436.004625	143.019429	50.144013
432.449744	143.828034	50.149018
428.996770	130.392261	50.154023
426.002076	137.507448	50.159028
422.319041	141.482627	50.164033
418.220757	133.506649	50.169037
415.028377	136.479839	50.174042
411.593657	150.389348	50.179047
408.580014	139.406461	50.184052
404.867250	138.038901	50.189057
401.382774	130.233034	50.194061
398.188374	135.776510	50.199066
393.852430	142.714228	50.204071
390.640781	135.033966	50.209076
387.010957	146.835703	50.214081
383.611326	132.292137	50.219085
380.452833	134.229398	50.224090
376.372761	141.173985	50.229095
373.289345	133.040543	50.234100
369.549545	135.021457	50.239105
366.141357	140.692904	50.244109
362.901317	131.000560	50.249114
358.999752	136.559859	50.254119
355.715229	133.445739	50.259124
352.049446	132.129247	50.264129
348.559712	131.185097	50.269133
345.425223	137.284679	50.274138
341.611677	129.077530	50.279143
338.163031	136.184976	50.284148
334.668351	136.433690	50.289153
331.026652	139.984386	50.294157
327.854525	118.076528	50.299162
323.879683	134.332696	50.304167
320.686246	136.907343	50.309172
316.914899	130.445832	50.314177
313.636891	131.006813	50.319181
310.234873	134.446792	50.324186
306.277097	136.349216	50.329191
303.096086	126.674684	50.334196
299.797969	130.721981	50.339201
295.883223	142.243395	50.344205
292.914721	132.062286	50.349210
289.359893	134.696359	50.354215
285.956092	118.349867	50.359220
281.863954	127.750320	50.364225
278.435368	137.015500	50.369229
274.964778	128.857393	50.374234
271.149463	126.819927	50.379239
268.005370	130.714233	50.384244
264.505269	123.886726	50.389249
260.884100	121.311194	50.394253
258.038273	124.996700	50.399258
254.173463	123.926045	50.404263
250.601769	127.555286	50.409268
246.765199	130.851139	50.414273
243.206484	137.297087	50.419277
240.363102	128.437628	50.424282
236.761634	141.120557	50.429287
233.288033	126.639339	50.434292
229.712119	126.756906	50.439297
226.104754	131.587940	50.444301
222.535154	134.210381	50.449306
218.526690	128.108149	50.454311
215.107726	128.868666	50.459316
212.085986	137.617678	50.464321
208.374559	129.604275	50.469325
205.291529	131.697652	50.474330
201.553145	143.787816	50.479335
197.723932	131.356219	50.484340
194.539710	127.200008	50.489345
191.059389	127.400850	50.494349
187.754452	127.278627	50.499354
183.973192	133.707509	50.504359
180.667389	135.104115	50.509364
177.058102	139.929969	50.514369
173.625876	131.959145	50.519373
170.096229	130.100359	50.524378
166.407583	132.469722	50.529383
162.869164	125.250738	50.534388
159.352937	126.115356	50.539393
155.471601	123.539961	50.544397
152.612851	121.617880	50.549402
148.965243	128.931425	50.554407
145.440687	120.292406	50.559412
141.980405	121.078534	50.564417
138.408805	128.748489	50.569421
135.033786	133.815436	50.574426
131.485502	135.810023	50.579431
128.052350	128.390958	50.584436
124.696643	129.300199	50.589441
121.058810	125.583807	50.594445
117.794741	129.409513	50.599450
113.731931	143.475502	50.604455
109.638523	127.276720	50.609460
106.667285	131.099719	50.614465
103.381370	138.854586	50.619469
100.228502	121.364891	50.624474
96.562955	122.527193	50.629479
92.818309	142.262645	50.634484
89.638567	129.486445	50.639489
85.964466	127.322370	50.644493
82.536425	124.742653	50.649498
78.589752	127.063941	50.654503
75.416670	130.983743	50.659508
71.943797	126.775954	50.664513
68.508786	128.629032	50.669517
65.079401	132.137680	50.674522
61.178276	141.049138	50.679527
57.861735	128.741087	50.684532
54.199520	129.432184	50.689537
50.935859	140.015950	50.694541
47.523868	127.137971	50.699546
43.590308	131.764926	50.704551
40.187320	137.924300	50.709556
36.921051	133.361072	50.714561
33.318276	134.362294	50.719565
29.904854	132.343208	50.724570
26.278876	127.000281	50.729575
22.915630	127.502888	50.734580
19.654113	130.629946	50.739585
15.538088	138.867126	50.744589
12.359113	129.998335	50.749594
8.705475	138.681379	50.754599
5.294849	145.961758	50.759604
2.290094	127.560549	50.764609