Thu Jun 16 11:29:01 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.224739	104.695007	0.000000
0.632760	106.867210	0.005005
0.813687	95.036953	0.010010
0.649253	108.357379	0.015014
0.850132	105.942375	0.020019
0.529671	93.815951	0.025024
0.226892	87.830848	0.030029
0.537299	78.684284	0.035034
0.185375	68.829542	0.040038
0.141768	58.938653	0.045043
-0.523626	41.906917	0.050048
-0.967160	44.252083	0.055053
-1.156895	31.967470	0.060058
-1.621868	30.669960	0.065062
-1.845851	21.040344	0.070067
-2.051471	30.586436	0.075072
-2.682286	25.757819	0.080077
-3.123413	18.069672	0.085082
-3.717546	22.889178	0.090086
-3.963721	21.951208	0.095091
-3.764224	23.539291	0.100096
-3.791234	33.582280	0.105101
-3.684184	23.699565	0.110106
-3.795559	25.051153	0.115110
-4.232057	15.150245	0.120115
-4.959437	25.883625	0.125120
-5.316668	33.039944	0.130125
-5.687112	30.165923	0.135130
-5.699417	35.192935	0.140134
-5.364520	24.730665	0.145139
-6.025158	31.217647	0.150144
-7.034248	39.750965	0.155149
-6.726343	24.783624	0.160154
-7.223310	38.095902	0.165158
-6.924961	27.377155	0.170163
-7.123617	27.978408	0.175168
-7.227104	32.728870	0.180173
-7.651381	30.860635	0.185178
-8.359851	30.226952	0.190182
-8.386364	30.885783	0.195187
-8.294483	33.112377	0.200192
-8.497556	27.940493	0.205197
-9.243912	27.171307	0.210202
-10.066302	28.115464	0.215206
-10.009306	25.650162	0.220211
-10.184755	24.024830	0.225216
-10.364908	39.117627	0.230221
-10.322559	31.030334	0.235226
-10.490137	30.268197	0.240230
-10.527475	32.302660	0.245235
-10.185016	23.796418	0.250240
-11.288795	24.617592	0.255245
-11.366604	28.509177	0.260250
-11.907219	29.011762	0.265254
-12.514018	21.738700	0.270259
-12.950606	27.354050	0.275264
-13.075610	24.429013	0.280269
-12.559904	26.117653	0.285274
-13.325177	41.249634	0.290278
-13.442270	40.405953	0.295283
-13.337725	22.161226	0.300288
-13.779991	27.430355	0.305293
-14.153312	38.213848	0.310298
-14.816463	32.256163	0.315302
-14.927110	32.516726	0.320307
-15.014032	16.650210	0.325312
-15.052362	32.977585	0.330317
-15.047571	34.481929	0.335322
-15.227460	37.672882	0.340326
-15.988200	36.043648	0.345331
-16.584279	39.084569	0.350336
-16.618183	39.434654	0.355341
-16.592778	23.452790	0.360346
-17.240171	35.191746	0.365350
-17.200573	30.312713	0.370355
-16.837472	23.437938	0.375360
-17.297691	27.150231	0.380365
-17.954447	29.424088	0.385370
-18.315274	28.324432	0.390374
-18.373816	30.841458	0.395379
-18.633663	24.755172	0.400384
-18.773780	35.465200	0.405389
-18.953331	35.274270	0.410394
-19.922352	24.450268	0.415398
-20.099607	26.536265	0.420403
-19.985155	28.760607	0.425408
-20.250040	32.550224	0.430413
-19.926777	25.286730	0.435418
-20.336934	33.081596	0.440422
-20.854320	32.956461	0.445427
-21.573019	34.479249	0.450432
-21.533926	37.075933	0.455437
-21.647469	29.903861	0.460442
-21.660302	40.846198	0.465446
-22.059760	35.314031	0.470451
-22.459574	25.846852	0.475456
-23.227405	32.133132	0.480461
-23.444054	31.256874	0.485466
-23.310575	34.376900	0.490470
-23.462013	15.573493	0.495475
-23.430791	41.603445	0.500480
-23.413111	44.036944	0.505485
-23.214420	36.902057	0.510490
-23.991838	36.301473	0.515494
-24.326151	28.294780	0.520499
-25.200697	34.210399	0.525504
-26.063752	39.345255	0.530509
-25.248761	38.886478	0.535514
-25.923806	40.147529	0.540518
-26.032677	34.212188	0.545523
-26.172650	35.121506	0.550528
-26.426455	47.711914	0.555533
-26.074362	34.150469	0.560538
-26.356962	44.656358	0.565542
-27.322006	36.822757	0.570547
-27.718946	37.404396	0.575552
-27.939579	40.655159	0.580557
-27.808260	40.648931	0.585562
-28.404496	33.441698	0.590566
-28.202639	39.722515	0.595571
-28.735549	32.148384	0.600576
-29.284168	32.713754	0.605581
-29.224623	27.335891	0.610586
-29.492580	33.884256	0.615590
-29.637182	48.844219	0.620595
-29.477339	35.667427	0.625600
-30.176944	36.126442	0.630605
-30.470196	40.086289	0.635610
-30.814388	45.786805	0.640614
-30.922694	36.123959	0.645619
-30.786251	33.785219	0.650624
-31.158639	42.892346	0.655629
-31.782957	37.334103	0.660634
-32.312543	40.723627	0.665638
-32.757888	43.381035	0.670643
-32.651345	39.034515	0.675648
-32.759204	35.408574	0.680653
-32.804967	29.118013	0.685658
-32.665976	41.457441	0.690662
-33.227640	41.669619	0.695667
-33.698029	33.050383	0.700672
-34.325714	41.238425	0.705677
-34.260265	29.470517	0.710682
-34.257645	34.901610	0.715686
-34.112155	37.073075	0.720691
-34.963315	33.203677	0.725696
-35.642157	29.407217	0.730701
-35.490424	25.953737	0.735706
-35.571166	41.338592	0.740710
-35.757412	26.065211	0.745715
-35.741370	24.265186	0.750720
-36.911199	45.503172	0.755725
-36.886449	35.303960	0.760730
-37.280574	39.006912	0.765734
-37.316872	38.197430	0.770739
-37.157811	40.898492	0.775744
-37.310012	37.335223	0.780749
-37.810023	24.707781	0.785754
-38.612200	40.946630	0.790758
-38.739499	36.093500	0.795763
-38.880521	32.855519	0.800768
-39.317686	44.881349	0.805773
-38.959082	23.972241	0.810778
-39.227008	27.619608	0.815782
-39.421439	41.056110	0.820787
-39.931105	29.322873	0.825792
-40.592461	26.233037	0.830797
-40.245093	27.778924	0.835802
-40.902231	43.871082	0.840806
-40.722379	43.514112	0.845811
-40.649903	29.405978	0.850816
-41.699188	40.976957	0.855821
-41.896796	31.741737	0.860826
-42.288439	23.072303	0.865830
-42.451770	35.100025	0.870835
-42.237867	34.290628	0.875840
-42.423378	29.422557	0.880845
-42.796868	30.007720	0.885850
-43.516781	47.895580	0.890854
-43.535053	36.716553	0.895859
-43.464545	31.980687	0.900864
-43.924673	40.779224	0.905869
-43.811222	40.340001	0.910874
-44.735726	41.553394	0.915878
-45.139879	35.228045	0.920883
-44.977339	29.450189	0.925888
-45.585561	36.021246	0.930893
-45.398195	36.736577	0.935898
-45.715590	34.804709	0.940902
-45.446185	36.516097	0.945907
-46.101293	34.540007	0.950912
-46.849462	48.274806	0.955917
-47.019128	32.191895	0.960922
-47.297098	39.888561	0.965926
-47.464177	33.951299	0.970931
-47.212153	34.504117	0.975936
-47.497360	40.062885	0.980941
-47.492547	35.458627	0.985946
-47.968041	43.902384	0.990950
-48.352520	52.207590	0.995955
-48.710948	39.580119	1.000960
-49.120015	38.795347	1.005965
-49.160796	42.545068	1.010970
-49.399443	51.395007	1.015974
-49.929833	41.063596	1.020979
-50.239716	36.712895	1.025984
-50.519772	44.063043	1.030989
-50.282989	34.779216	1.035994
-50.204575	47.466741	1.040998
-50.888284	38.673220	1.046003
-51.048155	36.522452	1.051008
-51.949029	48.656883	1.056013
-51.511903	38.503365	1.061018
-51.648721	31.149674	1.066022
-52.216910	46.137905	1.071027
-52.665257	35.843746	1.076032
-53.225495	29.521210	1.081037
-53.214108	33.175000	1.086042
-53.483870	41.235325	1.091046
-53.648162	38.115134	1.096051
-53.421068	35.516752	1.101056
-53.632149	30.736368	1.106061
-53.791416	31.190040	1.111066
-54.247084	31.034977	1.116070
-54.683817	37.032636	1.121075
-54.447109	23.699318	1.126080
-55.412509	43.816951	1.131085
-55.876920	42.215303	1.136090
-56.261443	33.993362	1.141094
-56.383205	36.432739	1.146099
-56.136488	36.377350	1.151104
-56.317952	36.906509	1.156109
-56.676029	31.444753	1.161114
-56.428319	31.162495	1.166118
-57.410014	36.354942	1.171123
-57.565254	41.579106	1.176128
-57.957930	42.519238	1.181133
-57.922210	37.429728	1.186138
-57.915962	31.290489	1.191142
-58.268348	43.738154	1.196147
-59.210452	34.025376	1.201152
-59.935956	30.124265	1.206157
-59.532923	36.118982	1.211162
-59.802392	36.080930	1.216166
-59.882143	54.133406	1.221171
-59.558354	33.176474	1.226176
-59.907460	46.093089	1.231181
-60.023495	36.343624	1.236186
-60.783099	28.185155	1.241190
-61.485816	33.875270	1.246195
-61.226228	38.276476	1.251200
-61.525939	43.154864	1.256205
-61.320318	33.762441	1.261210
-61.632278	45.054710	1.266214
-62.820332	40.481857	1.271219
-62.707249	37.704025	1.276224
-63.156297	53.443052	1.281229
-63.264641	42.911670	1.286234
-62.987754	43.470737	1.291238
-63.226513	45.808503	1.296243
-63.298288	34.201585	1.301248
-64.416234	32.403800	1.306253
-64.592587	31.594972	1.311258
-64.927310	40.312013	1.316262
-65.088026	44.255777	1.321267
-64.721471	28.158737	1.326272
-64.791053	31.765532	1.331277
-64.997912	34.033209	1.336282
-66.169105	38.465679	1.341286
-66.495961	40.061828	1.346291
-66.601503	34.236135	1.351296
-66.573052	41.435853	1.356301
-66.299812	24.501778	1.361306
-66.085127	33.647324	1.366310
-67.437849	37.007446	1.371315
-67.574359	33.361876	1.376320
-68.270565	42.970107	1.381325
-68.050288	28.938572	1.386330
-67.975024	20.498788	1.391334
-68.529682	27.849621	1.396339
-68.692850	28.164048	1.401344
-69.497383	40.199780	1.406349
-69.399682	21.733240	1.411354
-69.618442	37.885529	1.416358
-70.247126	42.994677	1.421363
-69.883057	25.535554	1.426368
-70.058428	26.123293	1.431373
-70.079543	39.711880	1.436378
-70.803261	32.216742	1.441382
-71.372026	39.225120	1.446387
-71.486738	22.690881	1.451392
-72.107468	30.459578	1.456397
-71.513502	33.464233	1.461402
-71.702289	33.290320	1.466406
-72.229950	42.580853	1.471411
-72.805587	29.008091	1.476416
-72.976584	33.840244	1.481421
-73.239282	36.038228	1.486426
-73.362605	34.471267	1.491430
-73.374554	29.377800	1.496435
-73.385116	28.573043	1.501440
-74.052513	41.546301	1.506445
-74.468210	19.583113	1.511450
-74.902631	41.968919	1.516454
-74.954600	30.080826	1.521459
-75.104452	27.484467	1.526464
-75.286414	37.748590	1.531469
-75.325447	33.105608	1.536474
-75.172320	36.753138	1.541478
-75.419795	41.778271	1.546483
-75.436454	31.357134	1.551488
-77.021720	39.153938	1.556493
-77.307860	37.573932	1.561498
-77.681562	41.472296	1.566502
-77.883486	47.790742	1.571507
-77.632270	37.995380	1.576512
-77.860127	40.464328	1.581517
-77.795320	36.037893	1.586522
-77.721076	36.167471	1.591526
-77.859509	41.200528	1.596531
-78.593957	30.839815	1.601536
-79.180776	32.967261	1.606541
-79.203583	35.696403	1.611546
-79.409961	46.848794	1.616550
-79.907193	34.996405	1.621555
-80.240412	33.491856	1.626560
-80.471203	34.019600	1.631565
-80.487166	31.494438	1.636570
-80.953292	37.388041	1.641574
-80.531435	48.019203	1.646579
-81.166750	39.589514	1.651584
-82.184862	35.943640	1.656589
-82.269233	47.588764	1.661594
-82.291278	47.248192	1.666598
-82.517689	40.823624	1.671603
-82.298320	44.119459	1.676608
-82.617199	42.624477	1.681613
-82.520765	42.043539	1.686618
-82.809267	44.694758	1.691622
-83.996667	44.469738	1.696627
-83.900616	34.561810	1.701632
-84.331158	45.674200	1.706637
-83.981433	39.995726	1.711642
-84.368676	39.509228	1.716646
-85.471542	55.018623	1.721651
-85.383354	39.129865	1.726656
-85.840838	34.825858	1.731661
-85.734130	40.726501	1.736666
-86.049777	33.703949	1.741670
-85.888245	51.445935	1.746675
-85.929061	33.850200	1.751680
-86.108488	48.278744	1.756685
-86.636576	38.150483	1.761690
-87.144517	35.527181	1.766694
-87.377640	43.117683	1.771699
-87.346671	33.394340	1.776704
-87.475535	36.403427	1.781709
-87.797234	34.402428	1.786714
-88.388573	35.116134	1.791718
-88.998037	36.454745	1.796723
-89.012378	35.306412	1.801728
-89.283257	35.558534	1.806733
-89.086136	30.368166	1.811738
-89.127256	33.367487	1.816742
-90.157496	30.914658	1.821747
-90.561267	30.565257	1.826752
-91.014995	36.890096	1.831757
-90.761555	21.777968	1.836762
-90.672138	38.852927	1.841766
-90.738877	35.292309	1.846771
-90.964080	32.807845	1.851776
-91.774279	32.498881	1.856781
-92.004432	32.403920	1.861786
-92.283531	27.862374	1.866790
-92.651445	39.338796	1.871795
-92.388139	31.004269	1.876800
-92.373224	37.615387	1.881805
-93.123517	35.702586	1.886810
-93.409417	36.674398	1.891814
-94.287303	31.574292	1.896819
-94.037724	31.251671	1.901824
-94.117510	34.999943	1.906829
-94.385164	24.306875	1.911834
-94.149639	30.579355	1.916838
-94.537218	42.140319	1.921843
-94.808321	24.851486	1.926848
-95.474253	32.535415	1.931853
-95.776573	42.735971	1.936858
-95.694894	41.813961	1.941862
-95.847544	32.939984	1.946867
-96.084600	27.017056	1.951872
-96.531093	41.252471	1.956877
-96.999168	32.592614	1.961882
-97.197006	28.600847	1.966886
-97.221096	34.875690	1.971891
-97.302491	30.519788	1.976896
-97.944437	30.954581	1.981901
-98.696050	37.149301	1.986906
-98.650657	42.634785	1.991910
-99.052460	41.253938	1.996915
-98.975898	38.733219	2.006912
-98.133405	36.175731	2.016909
-97.814649	36.904413	2.026906
-97.600848	37.323828	2.036902
-97.574397	33.019168	2.046899
-96.454529	34.773388	2.056896
-96.013447	38.292964	2.066893
-95.789277	31.325035	2.076890
-95.038437	37.439368	2.086886
-94.837041	35.224611	2.096883
-93.793660	27.474730	2.106880
-93.363253	32.781406	2.116877
-93.410849	27.406562	2.126874
-92.613924	36.980728	2.136870
-92.102218	38.773527	2.146867
-91.645459	28.475881	2.156864
-90.579456	34.474216	2.166861
-90.128367	37.892470	2.176858
-90.110573	32.628168	2.186854
-90.005956	24.435727	2.196851
-89.226010	30.324871	2.206848
-88.811993	31.364374	2.216845
-87.625240	33.613588	2.226842
-87.401554	42.753733	2.236838
-87.290539	41.187927	2.246835
-86.582616	35.914518	2.256832
-85.958003	34.005966	2.266829
-85.923994	40.649400	2.276826
-85.027045	43.671108	2.286822
-84.559696	36.875114	2.296819
-84.066090	34.772135	2.306816
-83.015840	35.272599	2.316813
-82.706944	32.425322	2.326810
-82.766344	33.412383	2.336806
-82.606577	39.897778	2.346803
-81.569213	35.618909	2.356800
-81.038839	32.855391	2.366797
-79.862794	37.971126	2.376794
-80.002058	37.092553	2.386790
-79.563008	28.716819	2.396787
-79.465220	35.040580	2.406784
-78.162581	36.192813	2.416781
-77.781072	35.971487	2.426778
-77.849773	37.930246	2.436774
-77.420128	35.173201	2.446771
-76.596922	28.720183	2.456768
-75.353802	37.850238	2.466765
-75.773644	35.862861	2.476762
-75.128960	34.962642	2.486758
-74.881393	34.822720	2.496755
-73.868385	33.919563	2.506752
-73.624191	30.574316	2.516749
-73.025807	41.599081	2.526746
-72.089310	44.001181	2.536742
-71.932341	33.941597	2.546739
-71.624056	36.530643	2.556736
-70.936668	31.749834	2.566733
-70.419140	36.660285	2.576730
-70.399961	45.939581	2.586726
-69.130238	34.670219	2.596723
-68.789601	38.807668	2.606720
-68.809751	36.317679	2.616717
-67.950366	33.031079	2.626714
-67.308705	32.275775	2.636710
-66.845726	38.252329	2.646707
-66.770759	38.205732	2.656704
-65.713241	39.376846	2.666701
-64.921692	31.053487	2.676698
-64.962427	41.191394	2.686694
-65.125606	39.727357	2.696691
-64.242471	33.765591	2.706688
-63.424816	37.259730	2.716685
-62.237423	43.608584	2.726682
-62.200791	31.565000	2.736678
-62.216466	35.732987	2.746675
-61.829977	27.061453	2.756672
-60.921278	30.072923	2.766669
-60.715870	35.920861	2.776666
-59.821815	39.048251	2.786662
-59.100061	37.311723	2.796659
-59.082466	35.232641	2.806656
-58.794380	31.979462	2.816653
-57.510763	28.591735	2.826650
-57.290534	32.790176	2.836646
-56.977913	33.969320	2.846643
-56.899670	37.606553	2.856640
-55.917547	42.056961	2.866637
-55.747091	36.546011	2.876634
-54.524246	29.904461	2.886630
-54.404491	31.130494	2.896627
-54.040287	33.847899	2.906624
-53.664100	39.211747	2.916621
-52.918164	32.879811	2.926618
-52.685219	34.781013	2.936614
-51.695023	38.558733	2.946611
-51.127937	30.557301	2.956608
-51.083497	31.648995	2.966605
-50.859569	33.136222	2.976602
-49.953114	31.315928	2.986598
-49.644369	31.668585	2.996595
-48.499520	27.414680	3.006592
-48.205921	30.877734	3.016589
-48.151258	34.723534	3.026586
-47.694922	38.682978	3.036582
-46.833999	37.389394	3.046579
-46.573132	34.442336	3.056576
-45.716186	29.580907	3.066573
-44.962421	35.120512	3.076570
-44.916661	36.136224	3.086566
-44.857668	36.622268	3.096563
-43.768400	31.499450	3.106560
-43.340037	37.535611	3.116557
-43.003393	34.040498	3.126554
-42.760002	33.578308	3.136550
-41.704461	35.730929	3.146547
-41.646877	33.233328	3.156544
-40.426879	36.498782	3.166541
-40.093159	35.202042	3.176538
-40.049099	33.673035	3.186534
-39.961466	26.295955	3.196531
-39.018071	34.204065	3.206528
-38.535443	34.532184	3.216525
-37.391249	28.823863	3.226522
-37.159382	39.113094	3.236518
-37.081007	40.003647	3.246515
-36.749931	32.159950	3.256512
-35.666740	31.201786	3.266509
-35.262918	34.446055	3.276506
-35.228697	32.783938	3.286502
-34.042692	36.413186	3.296499
-33.661487	30.401318	3.306496
-33.550774	36.707044	3.316493
-33.060189	31.404412	3.326490
-32.235858	31.892979	3.336486
-31.929713	35.591970	3.346483
-31.613395	37.002538	3.356480
-30.691447	37.789043	3.366477
-30.167385	42.267594	3.376474
-30.166206	38.499874	3.386470
-29.420128	36.267605	3.396467
-28.672018	30.961086	3.406464
-28.478938	34.422480	3.416461
-27.724997	30.530111	3.426458
-27.073402	40.397732	3.436454
-26.943232	31.313823	3.446451
-26.811872	29.710133	3.456448
-26.174381	30.386836	3.466445
-25.588459	26.940220	3.476442
-24.421204	33.633789	3.486438
-24.214434	35.564902	3.496435
-23.998755	26.878725	3.506432
-23.845941	36.141912	3.516429
-22.606283	37.181240	3.526426
-22.601610	31.799282	3.536422
-21.472392	40.301124	3.546419
-21.157868	39.978114	3.556416
-21.065734	37.636751	3.566413
-20.570075	38.783278	3.576410
-19.708400	27.594498	3.586406
-19.454342	34.386236	3.596403
-19.007107	34.808563	3.606400
-17.861301	37.259303	3.616397
-17.576199	30.628709	3.626394
-17.589264	36.598595	3.636390
-17.319441	34.235078	3.646387
-16.230099	39.027825	3.656384
-15.934148	35.490294	3.666381
-14.884048	34.775314	3.676378
-14.545620	35.863617	3.686374
-14.443086	34.576487	3.696371
-14.270162	35.630897	3.706368
-13.127956	29.818893	3.716365
-12.921753	32.629977	3.726362
-12.532486	34.800007	3.736358
-11.323166	32.153311	3.746355
-11.023651	34.432804	3.756352
-10.849472	31.990759	3.766349
-10.853548	31.221714	3.776346
-9.724900	28.701848	3.786342
-9.357851	35.097726	3.796339
-9.223341	29.540512	3.806336
-7.990427	33.115834	3.816333
-7.793095	31.451012	3.826330
-7.361588	23.577584	3.836326
-6.604438	34.811018	3.846323
-6.226191	32.573555	3.856320
-6.188604	26.299516	3.866317
-5.615204	36.328280	3.876314
-5.017376	35.758227	3.886310
-3.830866	30.938746	3.896307
-3.630138	37.260221	3.906304
-3.394312	30.418282	3.916301
-3.391980	45.869686	3.926298
-2.619941	53.618994	3.936294
-2.021125	56.529769	3.946291
-1.679316	73.021700	3.956288
-0.965952	74.766123	3.966285
-0.598447	88.022791	3.976282
-0.432130	105.031879	3.986278
0.000000	112.634933	3.991283
0.382558	115.019096	3.996288
1.012501	122.726176	4.001293
0.976690	130.437721	4.006298
0.785787	141.338924	4.011302
0.953291	154.962155	4.016307
0.977306	146.202545	4.021312
1.249216	125.685266	4.026317
0.838952	138.043331	4.031322
1.168137	133.056821	4.036326
0.842290	115.662767	4.041331
0.575249	141.214585	4.046336
1.103171	131.490533	4.051341
0.706892	141.521910	4.056346
0.973943	141.156349	4.061350
1.087878	130.435646	4.066355
0.764063	132.344624	4.071360
1.327756	140.999477	4.076365
0.832563	141.999566	4.081370
0.951332	134.506705	4.086374
1.176970	134.861353	4.091379
1.469381	148.825699	4.096384
1.236034	132.597128	4.101389
1.037912	130.138256	4.106394
1.140966	147.095281	4.111398
1.194830	141.706872	4.116403
1.100539	143.707058	4.121408
1.339098	135.356139	4.126413
0.925168	151.988402	4.131418
0.977798	134.082906	4.136422
0.914924	150.826740	4.141427
0.836410	137.553994	4.146432
1.170500	143.360381	4.151437
0.906617	146.541067	4.156442
1.493407	135.547278	4.161446
1.489579	147.234422	4.166451
1.010872	152.029270	4.171456
1.417385	141.781298	4.176461
1.198381	151.139175	4.181466
0.979752	152.574597	4.186470
1.366719	142.207524	4.191475
1.315859	158.971973	4.196480
1.787086	161.937656	4.201485
1.085147	155.827793	4.206490
1.401203	155.706588	4.211494
1.847384	165.606452	4.216499
1.232464	143.068279	4.221504
1.504071	145.072320	4.226509
1.132293	156.027003	4.231514
1.568738	143.589788	4.236518
1.690514	159.357224	4.241523
1.640329	167.425725	4.246528
1.914808	150.691269	4.251533
1.047305	145.094739	4.256538
1.457721	150.674141	4.261542
1.394835	144.415858	4.266547
1.313582	163.427932	4.271552
1.998915	159.792322	4.276557
1.474408	165.879710	4.281562
1.586201	160.964040	4.286566
1.631744	159.231437	4.291571
1.729185	155.599358	4.296576
1.460661	152.702256	4.301581
1.298167	159.566104	4.306586
1.408065	167.752087	4.311590
1.946787	165.327609	4.316595
1.723311	181.460318	4.321600
1.939027	170.633683	4.326605
2.090963	184.505753	4.331610
2.041977	169.975291	4.336614
1.293788	162.641866	4.341619
1.416073	156.856408	4.346624
1.814647	165.671745	4.351629
1.757646	179.592151	4.356634
1.643231	167.000599	4.361638
2.007781	178.772109	4.366643
1.655461	177.827697	4.371648
1.822210	173.411996	4.376653
1.746578	187.744902	4.381658
1.853703	185.745125	4.386662
2.007200	176.151092	4.391667
1.829464	168.060142	4.396672
1.806711	168.136497	4.401677
1.555340	184.331136	4.406682
1.658484	176.853267	4.411686
1.934059	176.681730	4.416691
1.442438	189.212804	4.421696
2.061202	171.979952	4.426701
2.063821	177.733992	4.431706
2.108506	183.057462	4.436710
2.071732	180.717433	4.441715
2.030002	176.614783	4.446720
2.239255	184.532393	4.451725
1.730068	193.942888	4.456730
1.668204	176.863451	4.461734
2.243881	182.072632	4.466739
1.688745	186.287506	4.471744
2.339644	180.794795	4.476749
1.926868	182.246223	4.481754
1.884655	188.787833	4.486758
2.080039	190.862485	4.491763
2.049041	192.240463	4.496768
2.248643	183.767902	4.501773
1.931742	183.509794	4.506778
1.981757	182.355548	4.511782
2.137812	180.716258	4.516787
2.033261	184.831708	4.521792
2.243909	174.969659	4.526797
2.049742	181.863119	4.531802
2.172066	179.536358	4.536806
1.950915	179.996116	4.541811
2.345755	194.151638	4.546816
2.436360	188.089056	4.551821
2.238264	176.955521	4.556826
2.156331	182.290642	4.561830
2.292990	191.495554	4.566835
2.060084	190.901261	4.571840
2.668297	197.970719	4.576845
1.709393	202.966381	4.581850
2.239895	200.847506	4.586854
2.619549	199.008384	4.591859
2.473603	215.326611	4.596864
2.714754	201.453155	4.601869
2.724742	201.157303	4.606874
2.408288	192.868279	4.611878
2.482085	180.298688	4.616883
1.958687	177.669717	4.621888
2.528171	182.671663	4.626893
2.786525	192.928144	4.631898
2.206135	181.692241	4.636902
2.343393	189.668415	4.641907
2.480585	201.582878	4.646912
2.745258	201.944987	4.651917
2.423692	199.162497	4.656922
2.492979	189.910496	4.661926
2.852760	200.277680	4.666931
2.125138	200.143186	4.671936
2.534180	196.937780	4.676941
2.587681	206.488217	4.681946
2.813303	198.878913	4.686950
2.635179	199.047338	4.691955
2.687625	197.727740	4.696960
2.660527	186.162445	4.701965
2.406762	190.634823	4.706970
2.449109	193.746267	4.711974
2.804948	211.044070	4.716979
2.873668	213.842273	4.721984
3.068145	196.510022	4.726989
2.533211	195.371645	4.731994
2.573868	184.097727	4.736998
2.699470	181.279521	4.742003
2.574671	202.966052	4.747008
2.845121	213.759692	4.752013
2.604126	204.958705	4.757018
3.124884	215.369638	4.762022
2.995924	200.197398	4.767027
2.620279	199.420802	4.772032
2.608743	185.377999	4.777037
2.564968	202.598488	4.782042
2.748377	211.946824	4.787046
2.897023	207.145999	4.792051
2.914846	207.130214	4.797056
3.053388	206.447702	4.802061
2.946472	216.704087	4.807066
2.733403	214.827858	4.812070
3.156845	204.834238	4.817075
2.856816	215.139306	4.822080
3.148526	201.714560	4.827085
3.231080	205.611160	4.832090
2.919026	202.483090	4.837094
2.520019	195.861348	4.842099
2.985042	204.712588	4.847104
3.097372	203.140798	4.852109
3.082746	205.930083	4.857114
2.713867	208.331106	4.862118
2.691974	210.939773	4.867123
2.527467	219.571667	4.872128
2.865562	203.968070	4.877133
2.942348	219.482062	4.882138
3.129304	220.261300	4.887142
3.227846	205.369717	4.892147
2.809090	215.879975	4.897152
2.870196	218.063933	4.902157
2.997608	208.987094	4.907162
2.944572	209.225610	4.912166
2.961545	231.597780	4.917171
2.911097	232.710439	4.922176
3.433437	229.536321	4.927181
3.273506	244.343631	4.932186
3.230398	233.374944	4.937190
3.185162	231.066987	4.942195
3.088962	242.032817	4.947200
3.292641	245.929240	4.952205
3.437952	237.228949	4.957210
3.700581	243.249524	4.962214
3.523428	214.770936	4.967219
3.060890	212.004341	4.972224
3.162210	214.324800	4.977229
3.200384	221.521423	4.982234
3.028618	232.519366	4.987238
3.229076	238.098672	4.992243
3.144683	254.194760	4.997248
3.242296	244.227831	5.002253
3.319178	239.774379	5.007258
3.414960	236.739119	5.012262
3.630426	240.042455	5.017267
3.617621	249.662674	5.022272
3.776142	250.682694	5.027277
3.645360	249.460358	5.032282
3.614346	241.909721	5.037286
3.596115	245.683687	5.042291
3.127355	240.834336	5.047296
3.403695	236.311322	5.052301
3.533380	243.613684	5.057306
3.410946	229.742674	5.062310
3.542730	234.504927	5.067315
3.843890	239.696158	5.072320
3.626827	231.081012	5.077325
3.385599	237.338751	5.082330
3.607910	243.698257	5.087334
3.625408	230.106497	5.092339
3.525796	235.371159	5.097344
3.987382	243.360947	5.102349
3.707489	235.303517	5.107354
3.291806	245.951206	5.112358
3.454059	241.955411	5.117363
3.512095	232.486230	5.122368
3.427172	227.003525	5.127373
3.527061	238.848021	5.132378
3.591909	241.756671	5.137382
3.421367	234.594118	5.142387
3.419891	246.553334	5.147392
3.507340	229.925368	5.152397
3.559330	240.806430	5.157402
3.969921	263.395848	5.162406
4.055263	246.443639	5.167411
3.484157	257.263227	5.172416
3.609229	252.690624	5.177421
3.946601	258.328208	5.182426
4.047972	277.518306	5.187430
4.109986	263.300004	5.192435
3.628282	241.292629	5.197440
3.856791	247.534010	5.202445
4.129394	265.939709	5.207450
3.699832	253.812048	5.212454
3.988469	252.080302	5.217459
3.890212	259.766420	5.222464
3.920330	251.033464	5.227469
4.232548	252.899006	5.232474
4.055167	248.422853	5.237478
4.006386	244.772201	5.242483
3.708409	247.488453	5.247488
3.786099	245.327991	5.252493
3.925796	253.768655	5.257498
3.979029	261.168404	5.262502
4.319739	269.102020	5.267507
4.061808	273.168554	5.272512
4.121402	264.535984	5.277517
4.134494	268.489854	5.282522
3.759108	280.746180	5.287526
4.088608	264.739359	5.292531
3.980212	257.415189	5.297536
3.960666	267.338219	5.302541
3.839958	267.476537	5.307546
3.559244	266.739595	5.312550
4.364496	271.019623	5.317555
3.907950	276.756253	5.322560
3.802355	261.670459	5.327565
4.059987	271.106206	5.332570
3.666626	273.509509	5.337574
4.209340	285.189408	5.342579
4.521224	300.350711	5.347584
4.708920	290.738327	5.352589
4.348980	286.943256	5.357594
4.087004	278.595361	5.362598
3.886426	265.466192	5.367603
4.211037	285.961210	5.372608
4.041223	290.484362	5.377613
4.276307	297.635753	5.382618
4.161787	296.710636	5.387622
4.777969	295.234926	5.392627
4.667982	305.345869	5.397632
4.488385	293.357505	5.402637
4.424821	283.009644	5.407642
4.426205	293.832613	5.412646
4.682950	286.389782	5.417651
4.117703	280.014785	5.422656
4.504382	292.475282	5.427661
4.204188	294.073756	5.432666
4.110256	294.249184	5.437670
4.706247	284.357419	5.442675
4.408547	302.320628	5.447680
4.193910	304.096552	5.452685
4.612658	292.907166	5.457690
4.455508	293.587499	5.462694
4.507727	291.972360	5.467699
4.302142	304.971039	5.472704
4.524201	295.729835	5.477709
4.457321	300.316679	5.482714
4.425704	302.950448	5.487718
4.370714	303.590714	5.492723
4.479116	304.775684	5.497728
4.453714	304.387813	5.502733
4.606398	298.586031	5.507738
4.279392	293.169353	5.512742
4.521543	316.151018	5.517747
4.814370	326.296922	5.522752
4.907494	313.540925	5.527757
4.700337	310.058197	5.532762
4.647758	299.051862	5.537766
4.619515	300.411144	5.542771
4.800604	325.428296	5.547776
4.798258	318.882519	5.552781
4.520026	314.381677	5.557786
4.503738	319.689325	5.562790
5.264753	328.973651	5.567795
4.816698	331.113220	5.572800
5.074893	325.311158	5.577805
4.697036	316.688796	5.582810
4.646652	312.269180	5.587814
4.852403	326.777788	5.592819
4.607449	330.045455	5.597824
5.096660	332.312781	5.602829
5.015106	328.759077	5.607834
4.978854	328.184370	5.612838
4.585594	330.431592	5.617843
4.613204	329.653461	5.622848
5.197757	336.456875	5.627853
4.623051	338.017059	5.632858
4.603762	324.209716	5.637862
5.268314	335.454675	5.642867
4.793146	343.824846	5.647872
4.636433	320.503135	5.652877
4.978480	331.848938	5.657882
4.820761	336.907676	5.662886
4.841538	329.857004	5.667891
4.842017	337.255247	5.672896
5.060290	336.947663	5.677901
5.321505	344.156022	5.682906
4.890229	331.743273	5.687910
5.113153	333.660281	5.692915
4.812777	336.813198	5.697920
5.003573	341.688163	5.702925
5.260091	364.963491	5.707930
5.208713	361.410416	5.712934
5.440599	346.871155	5.717939
4.940583	346.529062	5.722944
4.856587	345.076223	5.727949
5.509607	348.856388	5.732954
5.291112	360.312505	5.737958
5.295380	354.296977	5.742963
5.415936	362.325132	5.747968
5.619930	339.850916	5.752973
5.305666	333.669810	5.757978
5.091050	347.881600	5.762982
5.286296	339.620203	5.767987
5.062283	334.818672	5.772992
5.128716	335.327295	5.777997
5.357527	351.027024	5.783002
5.385977	363.044328	5.788006
5.250243	361.650450	5.793011
5.459773	370.433514	5.798016
5.492831	360.123302	5.803021
5.435541	374.158371	5.808026
5.107197	381.638205	5.813030
5.270455	365.891776	5.818035
5.426015	369.162421	5.823040
5.572182	357.570041	5.828045
5.278835	358.702823	5.833050
5.413108	372.804692	5.838054
5.978450	367.154198	5.843059
5.898938	367.221189	5.848064
5.436627	351.311686	5.853069
5.495989	350.704603	5.858074
5.147074	345.868167	5.863078
5.463079	345.516709	5.868083
5.294171	356.338268	5.873088
5.518885	361.618928	5.878093
5.775065	358.551810	5.883098
5.731159	363.818260	5.888102
5.442012	369.778733	5.893107
5.532121	369.585163	5.898112
5.544442	376.306863	5.903117
5.425335	363.785970	5.908122
5.488686	366.408199	5.913126
5.497338	367.178337	5.918131
5.706581	368.723905	5.923136
5.745508	360.070821	5.928141
5.474727	377.529980	5.933146
5.240004	379.363493	5.938150
5.378834	370.894164	5.943155
5.332435	364.912063	5.948160
5.490523	392.168850	5.953165
5.610615	388.111518	5.958170
5.727426	396.697712	5.963174
5.934179	390.826386	5.968179
5.737631	404.518485	5.973184
5.687875	395.629748	5.978189
5.645568	397.195579	5.983194
5.532693	399.851179	5.988198
6.273513	394.661303	5.993203
5.789299	399.787434	5.998208
5.748414	385.769325	6.003213
5.870416	397.361973	6.008218
5.995434	399.590248	6.013222
6.089270	386.076004	6.018227
5.774747	396.272601	6.023232
5.899201	405.749284	6.028237
5.900962	395.219088	6.033242
6.145750	404.296257	6.038246
6.100651	394.426017	6.043251
5.795284	397.463555	6.048256
5.510118	401.867882	6.053261
6.219175	390.129083	6.058266
5.920213	391.775014	6.063270
6.081288	384.132088	6.068275
6.037013	385.483273	6.073280
5.578137	378.755919	6.078285
5.811772	377.235393	6.083290
5.589631	391.657616	6.088294
6.009611	384.041555	6.093299
5.967471	398.783179	6.098304
5.934962	387.422547	6.103309
6.018537	377.945209	6.108314
5.735333	388.967402	6.113318
5.868279	370.549851	6.118323
5.558832	382.968008	6.123328
6.120808	388.173112	6.128333
6.066093	388.716260	6.133338
5.644298	383.036612	6.138342
5.884806	371.742946	6.143347
5.689953	376.152960	6.148352
5.721273	386.700239	6.153357
5.727562	394.887187	6.158362
5.713483	396.526883	6.163366
5.974801	390.150007	6.168371
5.725029	394.641416	6.173376
6.283335	395.496920	6.178381
5.945042	391.829852	6.183386
5.639960	389.001194	6.188390
6.148582	382.964164	6.193395
5.758762	389.907117	6.198400
5.908330	369.005639	6.203405
5.912233	375.372585	6.208410
5.739109	379.152351	6.213414
6.334716	370.171184	6.218419
5.467868	370.581876	6.223424
5.659048	372.958048	6.228429
6.060173	378.884166	6.233434
5.766909	377.971515	6.238438
5.955164	372.950110	6.243443
5.493758	382.846198	6.248448
5.888624	390.261965	6.253453
6.003748	386.377706	6.258458
5.627952	393.493555	6.263462
5.889136	396.593145	6.268467
5.784106	405.588330	6.273472
5.908200	390.350504	6.278477
5.825154	390.016552	6.283482
5.885557	403.178731	6.288486
5.579268	393.866143	6.293491
5.921317	401.054660	6.298496
6.006188	402.723879	6.303501
6.430666	395.328748	6.308506
6.075253	386.586815	6.313510
5.937862	372.673950	6.318515
5.687885	375.557603	6.323520
5.567509	365.280833	6.328525
5.756998	372.137316	6.333530
5.693613	381.020538	6.338534
5.803277	390.205464	6.343539
5.862549	398.046553	6.348544
5.768563	397.661726	6.353549
6.325298	393.544073	6.358554
6.010690	381.487781	6.363558
5.712508	360.211428	6.368563
6.010770	371.077435	6.373568
6.126629	359.686386	6.378573
6.319700	355.040659	6.383578
5.986892	370.241781	6.388582
5.964984	363.919318	6.393587
5.997643	360.608464	6.398592
5.765294	365.238654	6.403597
6.205469	354.201854	6.408602
5.693742	361.048626	6.413606
6.023571	363.731786	6.418611
5.655409	368.874048	6.423616
5.737851	363.351205	6.428621
5.837862	367.018745	6.433626
5.590435	368.595681	6.438630
5.691681	348.970331	6.443635
5.629800	364.206882	6.448640
5.585658	371.111149	6.453645
6.104588	357.129791	6.458650
5.783539	368.581454	6.463654
5.931670	362.325502	6.468659
5.740991	354.016591	6.473664
5.689230	355.518868	6.478669
5.946578	371.784228	6.483674
5.531806	369.533175	6.488678
5.775561	361.311993	6.493683
5.720838	370.500200	6.498688
5.889052	377.298147	6.503693
6.266649	376.029770	6.508698
5.611159	370.814937	6.513702
5.621016	360.167606	6.518707
6.000286	385.456950	6.523712
5.943253	374.484545	6.528717
6.003602	357.993412	6.533722
5.832065	364.164708	6.538726
5.936206	360.936257	6.543731
5.710530	365.686395	6.548736
5.396926	375.130678	6.553741
5.816207	384.240166	6.558746
6.004794	392.144824	6.563750
6.134077	390.786861	6.568755
5.882164	373.582736	6.573760
5.485557	364.271576	6.578765
5.800646	382.894737	6.583770
5.809671	392.371051	6.588774
6.077707	389.884626	6.593779
6.289758	385.258148	6.598784
6.225338	370.130321	6.603789
6.033349	355.173152	6.608794
6.061248	369.945498	6.613798
6.065829	360.897747	6.618803
5.962610	375.781246	6.623808
6.240278	377.564118	6.628813
6.206845	364.406255	6.633818
5.623941	377.103213	6.638822
5.964730	361.901426	6.643827
6.060553	368.717548	6.648832
5.586691	367.112489	6.653837
5.758962	364.567409	6.658842
5.699316	364.908535	6.663846
5.931730	366.836607	6.668851
5.623592	372.475151	6.673856
5.761589	364.627688	6.678861
5.804611	363.520163	6.683866
5.792506	366.644883	6.688870
5.837581	360.508563	6.693875
5.752534	369.280523	6.698880
5.649160	365.853734	6.703885
5.839125	353.445738	6.708890
5.445736	364.518087	6.713894
5.709790	368.064104	6.718899
5.685220	364.497127	6.723904
5.829939	368.207198	6.728909
5.953910	370.102285	6.733914
5.920513	368.399771	6.738918
5.745802	368.509526	6.743923
5.527032	368.871918	6.748928
5.481515	358.994666	6.753933
6.136086	385.367920	6.758938
5.980818	386.392055	6.763942
5.870940	368.520836	6.768947
6.055225	369.833755	6.773952
5.592914	365.114905	6.778957
5.689111	368.166677	6.783962
5.732505	378.324634	6.788966
6.195394	384.668612	6.793971
5.935214	372.955532	6.798976
5.814170	360.814094	6.803981
5.891481	356.031029	6.808986
5.676711	369.516269	6.813990
5.726444	361.756399	6.818995
5.824901	381.847043	6.824000
6.143244	394.900193	6.829005
6.036907	374.541082	6.834010
5.792620	368.483359	6.839014
6.095118	359.822925	6.844019
5.683480	359.857097	6.849024
5.833900	366.120606	6.854029
5.860115	363.620381	6.859034
5.572301	373.316412	6.864038
5.627132	361.669176	6.869043
6.030978	385.212503	6.874048
5.889549	379.017024	6.879053
6.220666	370.158391	6.884058
5.581189	374.252391	6.889062
5.526275	370.300147	6.894067
5.348722	377.593856	6.899072
5.644231	393.590313	6.904077
6.327917	393.434794	6.909082
6.253913	389.311276	6.914086
6.332369	386.311702	6.919091
6.084695	386.663283	6.924096
5.546970	377.909359	6.929101
5.748734	360.412741	6.934106
5.447939	370.272709	6.939110
6.026612	384.069111	6.944115
5.850587	381.693068	6.949120
5.836778	375.250086	6.954125
6.067517	379.396700	6.959130
5.717045	374.361031	6.964134
5.788869	365.104558	6.969139
5.753271	378.565524	6.974144
5.952720	379.604044	6.979149
5.868259	367.665507	6.984154
5.704015	369.819642	6.989158
5.836015	384.488474	6.994163
5.963884	391.987926	6.999168
6.293056	394.070192	7.004173
6.321060	383.743435	7.009178
5.993127	371.732958	7.014182
5.611075	376.818917	7.019187
5.542299	366.373994	7.024192
5.472638	372.616656	7.029197
5.917730	371.392865	7.034202
5.721443	369.663108	7.039206
5.747744	365.433343	7.044211
5.961170	382.062710	7.049216
5.889515	389.727725	7.054221
5.862112	378.304400	7.059226
5.865313	379.339934	7.064230
5.622256	375.576333	7.069235
6.306022	386.169297	7.074240
6.034567	377.151566	7.079245
5.692903	376.995313	7.084250
5.348166	372.224967	7.089254
5.861382	386.721986	7.094259
6.155284	395.241326	7.099264
6.156294	375.617906	7.104269
6.058441	374.057748	7.109274
5.999973	367.817190	7.114278
5.965188	366.299490	7.119283
5.899643	364.387616	7.124288
5.870361	373.075581	7.129293
6.233523	363.941835	7.134298
6.028776	372.470760	7.139302
6.079791	366.286595	7.144307
5.775585	370.764006	7.149312
5.677542	361.178772	7.154317
5.665795	366.638995	7.159322
5.678397	375.812133	7.164326
6.035976	358.511051	7.169331
5.986067	366.799514	7.174336
5.816516	378.594330	7.179341
5.723201	353.532861	7.184346
5.612925	365.041932	7.189350
5.750973	368.307776	7.194355
6.104202	363.672969	7.199360
5.580006	364.474339	7.204365
5.647606	363.854549	7.209370
5.376260	374.497909	7.214374
5.411295	362.790409	7.219379
5.684114	378.314095	7.224384
5.498033	394.692122	7.229389
5.552266	392.583265	7.234394
5.538839	393.235510	7.239398
6.098063	394.936437	7.244403
6.033553	396.891581	7.249408
5.989071	393.119034	7.254413
6.430208	391.815689	7.259418
6.313832	408.409514	7.264422
6.146066	377.533618	7.269427
5.837223	372.089148	7.274432
5.813288	368.519598	7.279437
5.964052	363.710088	7.284442
5.872168	373.570656	7.289446
6.016404	367.781195	7.294451
5.946950	362.839279	7.299456
5.951216	372.173317	7.304461
5.774012	368.386207	7.309466
5.675412	365.720544	7.314470
6.299173	362.040507	7.319475
6.020020	363.408111	7.324480
5.778623	377.591304	7.329485
6.087111	354.738621	7.334490
6.025014	361.669529	7.339494
5.760726	361.297555	7.344499
6.071603	369.356020	7.349504
5.570750	364.844499	7.354509
6.012161	354.171828	7.359514
5.825760	362.720801	7.364518
5.843844	366.146363	7.369523
5.864538	363.378017	7.374528
5.646184	363.430168	7.379533
6.035995	372.429191	7.384538
5.770406	364.756057	7.389542
5.847033	361.968405	7.394547
5.852702	377.810500	7.399552
5.875531	371.807485	7.404557
5.918695	359.933594	7.409562
6.000120	380.890382	7.414566
5.860224	368.854654	7.419571
5.764209	364.830279	7.424576
5.321850	372.087442	7.429581
5.654260	367.342325	7.434586
5.619355	371.121050	7.439590
6.204184	376.550958	7.444595
6.166563	363.661933	7.449600
5.983723	373.530330	7.454605
6.137460	367.414033	7.459610
5.848438	377.020588	7.464614
5.844586	368.280748	7.469619
5.998250	368.029616	7.474624
5.917616	372.034913	7.479629
6.046897	364.605315	7.484634
5.831406	370.230224	7.489638
5.739508	365.722251	7.494643
6.035217	367.028102	7.499648
5.941266	373.305262	7.504653
6.306492	363.282093	7.509658
5.983657	345.787638	7.514662
5.792398	337.078885	7.519667
5.720386	342.726835	7.524672
5.664527	364.826024	7.529677
5.763276	356.336590	7.534682
5.732470	368.932734	7.539686
5.733694	368.808310	7.544691
5.928549	364.656351	7.549696
5.497123	375.809873	7.554701
6.019512	362.981218	7.559706
6.097112	362.876433	7.564710
5.668858	371.140803	7.569715
5.486210	359.296929	7.574720
5.611557	380.849538	7.579725
5.771901	374.313255	7.584730
5.674120	372.644565	7.589734
5.717954	368.067793	7.594739
5.738015	374.572947	7.599744
5.707973	366.827343	7.604749
5.910899	368.351856	7.609754
5.665017	379.100025	7.614758
5.917875	370.514677	7.619763
5.569060	373.519533	7.624768
5.655506	378.236839	7.629773
5.915483	371.972955	7.634778
5.524171	369.667514	7.639782
5.710175	386.919591	7.644787
5.989650	393.637993	7.649792
6.265614	398.963767	7.654797
6.212999	385.772948	7.659802
5.962135	364.101744	7.664806
5.974637	370.868695	7.669811
6.173084	367.989977	7.674816
5.823050	369.643853	7.679821
5.892461	372.355253	7.684826
6.027432	371.013419	7.689830
6.001203	368.680794	7.694835
5.788592	362.587551	7.699840
5.633624	373.390342	7.704845
5.885867	370.851283	7.709850
5.705371	374.931488	7.714854
6.138219	374.995001	7.719859
5.771481	374.141255	7.724864
5.372730	367.121322	7.729869
5.843760	366.563213	7.734874
5.830574	375.482727	7.739878
6.135141	367.843127	7.744883
5.972559	375.473243	7.749888
5.781317	383.364207	7.754893
6.107925	373.663802	7.759898
5.772331	371.984098	7.764902
5.745383	372.659392	7.769907
5.874581	371.750129	7.774912
6.020752	376.777504	7.779917
6.092212	365.513357	7.784922
6.047000	372.440690	7.789926
6.138891	366.349807	7.794931
6.049413	377.997810	7.799936
5.621231	383.596213	7.804941
5.910531	378.946218	7.809946
6.004352	375.365888	7.814950
5.997634	375.124686	7.819955
6.329094	367.984080	7.824960
5.512658	357.878676	7.829965
5.821498	364.866967	7.834970
5.483558	369.620071	7.839974
5.712772	374.157512	7.844979
6.064995	371.046896	7.849984
5.907161	370.843591	7.854989
5.765860	362.855729	7.859994
5.876295	374.069659	7.864998
5.797575	366.540657	7.870003
5.772704	366.947364	7.875008
5.679408	371.271634	7.880013
5.980114	363.407740	7.885018
5.841071	366.386808	7.890022
5.970112	362.837854	7.895027
6.004061	364.285914	7.900032
5.705458	372.742941	7.905037
6.116797	362.872566	7.910042
5.847187	366.087391	7.915046
5.999830	364.826396	7.920051
5.970693	367.539184	7.925056
5.523503	363.570771	7.930061
5.521466	364.869297	7.935066
5.608110	368.967013	7.940070
5.646989	365.822942	7.945075
5.791388	369.378474	7.950080
5.578599	369.310430	7.955085
5.686606	370.455416	7.960090
5.996317	374.205506	7.965094
6.149401	378.031400	7.970099
6.047220	373.436827	7.975104
5.525236	371.846921	7.980109
5.793158	364.735561	7.985114
5.854707	386.713566	7.990118
5.799287	368.759118	7.995136
6.076005	363.253847	8.000154
5.370487	377.074796	8.005171
5.947844	366.997112	8.010189
5.797565	369.993425	8.015206
5.920544	371.954050	8.020224
5.934554	374.461406	8.025242
5.926112	360.916947	8.030259
6.033435	362.362555	8.035277
5.776728	371.622720	8.040294
5.688967	367.276357	8.045312
6.248743	372.039462	8.050330
5.668298	367.290273	8.055347
5.947148	373.861916	8.060365
6.052554	369.601615	8.065382
6.017935	378.497596	8.070400
6.385357	359.620624	8.075418
5.571031	359.388630	8.080435
6.151996	362.024092	8.085453
5.915542	364.197034	8.090470
5.638009	365.465942	8.095488
6.090668	379.447485	8.100506
6.105031	380.463772	8.105523
5.841954	364.930830	8.110541
5.930567	366.980186	8.115558
5.899290	366.347981	8.120576
5.931878	363.986505	8.125594
5.532547	378.543199	8.130611
5.934183	365.866686	8.135629
5.678588	365.149039	8.140646
5.988409	376.458912	8.145664
6.051267	367.142482	8.150682
6.274868	373.232222	8.155699
6.018366	373.570299	8.160717
5.912767	374.885188	8.165734
5.765042	372.735949	8.170752
6.053367	377.709430	8.175770
5.926624	380.125210	8.180787
6.227534	396.008404	8.185805
5.999995	395.834522	8.190822
5.996450	386.989486	8.195840
6.502408	404.090989	8.200858
6.095727	389.597970	8.205875
6.041924	370.156777	8.210893
5.953282	372.567244	8.215910
5.923696	373.519253	8.220928
6.367463	369.084657	8.225946
5.719388	381.016805	8.230963
6.021718	385.179981	8.235981
6.561014	390.678403	8.240998
5.971667	391.123345	8.246016
6.014486	383.467040	8.251034
5.672023	381.700595	8.256051
6.214656	397.447801	8.261069
6.269577	401.751256	8.266086
6.132230	397.910214	8.271104
6.394618	404.230611	8.276122
6.375700	411.342612	8.281139
6.147727	392.373286	8.286157
5.635421	378.463751	8.291174
5.935779	395.820335	8.296192
6.419008	408.451772	8.301210
6.284627	406.175449	8.306227
6.286656	404.193050	8.311245
6.477841	401.994196	8.316262
6.183692	390.486453	8.321280
5.745356	372.612315	8.326298
6.059991	385.239219	8.331315
6.066257	397.246965	8.336333
6.469780	403.399680	8.341350
6.035293	409.032759	8.346368
6.343483	406.869871	8.351386
5.897057	413.369796	8.356403
6.317314	408.838111	8.361421
6.379907	407.894983	8.366438
6.318027	401.329952	8.371456
6.256183	395.347270	8.376474
6.201436	398.703901	8.381491
6.595249	400.115355	8.386509
6.764227	405.094102	8.391526
6.130327	392.996384	8.396544
6.186981	382.554543	8.401562
6.251016	384.849151	8.406579
6.312004	391.121347	8.411597
6.347887	394.292859	8.416614
6.218427	391.894885	8.421632
6.296811	385.205227	8.426650
6.365119	394.100640	8.431667
6.356875	399.709624	8.436685
6.289310	388.363706	8.441702
6.400906	392.902227	8.446720
6.474473	378.840372	8.451738
6.368396	377.688754	8.456755
6.040796	368.709723	8.461773
6.349144	380.658875	8.466790
6.553808	395.987922	8.471808
6.433420	385.905186	8.476826
6.242493	379.689666	8.481843
6.237190	385.627221	8.486861
6.241912	386.261130	8.491878
6.182248	404.721087	8.496896
6.473062	397.950559	8.501914
6.678104	405.054379	8.506931
6.787647	398.033554	8.511949
6.530710	383.720867	8.516966
5.765026	376.760751	8.521984
6.161198	383.525758	8.527002
6.507330	388.933785	8.532019
6.477458	393.826814	8.537037
6.514635	390.891276	8.542054
6.174332	404.985385	8.547072
6.264998	398.182889	8.552090
5.975869	403.627217	8.557107
5.989757	409.826808	8.562125
6.514234	402.058128	8.567143
6.161610	390.810584	8.572160
6.245888	398.470953	8.577178
6.057106	402.081771	8.582195
6.309217	395.589924	8.587213
6.862316	418.126266	8.592231
6.560275	431.651108	8.597248
6.227841	402.887766	8.602266
6.019373	407.623149	8.607283
6.260137	431.719658	8.612301
6.776007	426.787997	8.617319
6.689657	438.481625	8.622336
6.796397	422.952751	8.627354
6.364319	434.820511	8.632371
6.563579	427.722064	8.637389
6.842908	416.030672	8.642407
6.651606	438.766522	8.647424
6.802822	425.689609	8.652442
6.408695	410.990601	8.657459
6.435766	415.713927	8.662477
6.422645	407.983113	8.667495
6.387957	421.768325	8.672512
6.829961	429.890838	8.677530
7.187759	426.873377	8.682547
6.383747	412.604526	8.687565
6.852307	406.324095	8.692583
6.282027	407.220020	8.697600
6.554761	398.184273	8.702618
6.327823	412.408047	8.707635
6.624645	423.004313	8.712653
6.889566	422.618762	8.717671
6.434968	423.959053	8.722688
6.865171	425.726228	8.727706
6.637812	420.176609	8.732723
6.473677	426.945077	8.737741
6.722707	425.761242	8.742759
6.545558	424.501412	8.747776
6.561294	436.512445	8.752794
6.535292	433.309250	8.757811
6.986045	434.874254	8.762829
7.030448	432.790185	8.767847
6.635954	431.403806	8.772864
6.792014	410.987926	8.777882
6.795832	416.819284	8.782899
6.668497	411.839625	8.787917
6.792783	401.934704	8.792935
6.363603	409.093444	8.797952
6.535358	423.258526	8.802970
6.778209	419.317746	8.807987
6.583797	434.648131	8.813005
6.569964	421.935628	8.818023
6.474089	429.565265	8.823040
6.893983	417.292299	8.828058
6.862505	438.331921	8.833075
6.993260	426.280904	8.838093
6.903022	420.904154	8.843111
6.803407	429.415911	8.848128
6.833223	436.675545	8.853146
6.855928	434.938884	8.858163
6.641544	440.982552	8.863181
6.844600	440.251986	8.868199
6.703868	436.436291	8.873216
6.912810	427.744855	8.878234
6.877237	431.071362	8.883251
6.654094	433.484679	8.888269
6.926763	429.012902	8.893287
7.046339	431.667452	8.898304
6.782461	426.275604	8.903322
6.901701	431.352226	8.908339
6.729389	433.925513	8.913357
7.363992	426.733376	8.918375
7.058124	435.531923	8.923392
6.933744	415.231559	8.928410
6.787797	405.923438	8.933427
6.481197	414.237356	8.938445
6.724998	426.398152	8.943463
6.701770	437.169733	8.948480
6.496951	432.549254	8.953498
6.912553	428.374555	8.958515
6.834537	435.095042	8.963533
6.759676	429.701183	8.968551
6.834650	444.123072	8.973568
6.727630	431.325097	8.978586
6.921205	425.824983	8.983603
6.596925	438.282773	8.988621
6.983919	429.617509	8.993639
7.000778	435.461382	8.998656
6.762044	442.362926	9.003674
7.052135	432.544044	9.008691
6.949893	434.191677	9.013709
7.131916	436.628472	9.018727
7.018551	440.460250	9.023744
6.673110	428.212690	9.028762
6.967443	428.868313	9.033779
6.909843	433.039813	9.038797
6.701883	434.452806	9.043815
7.005472	462.862065	9.048832
7.182909	456.939107	9.053850
6.990556	461.494913	9.058867
7.239670	463.054275	9.063885
7.469565	460.886409	9.068903
7.020472	455.478516	9.073920
6.830915	439.532450	9.078938
7.214228	428.471855	9.083955
6.923449	443.109959	9.088973
7.248480	434.887222	9.093991
7.312228	440.167069	9.099008
7.218857	443.363790	9.104026
7.346718	440.800279	9.109043
7.114647	432.182803	9.114061
6.924395	431.959953	9.119079
6.778997	431.068122	9.124096
6.752854	428.717621	9.129114
6.981054	442.191354	9.134131
6.925011	469.835531	9.139149
7.185533	460.488250	9.144167
6.909760	459.087760	9.149184
7.219607	457.286817	9.154202
7.647369	459.246977	9.159219
7.213134	471.190992	9.164237
7.436768	458.098935	9.169255
7.205734	464.493517	9.174272
6.960672	459.615171	9.179290
7.193960	470.483921	9.184307
7.042578	473.555223	9.189325
7.248031	458.668915	9.194343
7.609432	466.458090	9.199360
7.165243	468.289669	9.204378
7.330805	451.975718	9.209395
7.199436	456.934348	9.214413
7.129588	461.166333	9.219431
7.305924	467.753875	9.224448
7.157300	474.301343	9.229466
7.496884	475.919066	9.234483
7.358893	462.209548	9.239501
6.897683	457.301287	9.244519
7.294649	462.867538	9.249536
7.521336	456.311476	9.254554
7.420031	460.367595	9.259571
7.069705	460.942490	9.264589
7.110160	464.202120	9.269607
7.089525	465.305675	9.274624
6.890191	467.362973	9.279642
7.008668	462.113394	9.284659
7.004424	472.506352	9.289677
7.057602	471.477295	9.294695
7.012162	466.791598	9.299712
6.892866	473.869537	9.304730
7.332423	486.659701	9.309747
7.437663	491.261591	9.314765
7.650955	492.882376	9.319783
7.614702	487.033393	9.324800
7.253966	491.581609	9.329818
7.081535	467.546209	9.334835
7.371649	476.507946	9.339853
7.367574	489.196069	9.344871
7.504299	502.860329	9.349888
7.523458	499.480204	9.354906
7.677042	489.833912	9.359923
7.442677	484.372515	9.364941
7.256910	474.164530	9.369959
7.471032	464.641784	9.374976
7.512520	474.309819	9.379994
7.504370	463.512077	9.385011
7.496163	462.048673	9.390029
7.234769	465.011705	9.395047
7.549991	484.088793	9.400064
7.409147	481.079627	9.405082
7.609372	473.797476	9.410099
7.395818	490.063853	9.415117
7.612409	477.756536	9.420135
7.495716	473.873192	9.425152
7.242926	486.762813	9.430170
7.954141	488.190608	9.435187
7.812878	480.394633	9.440205
7.418160	467.863319	9.445223
7.764446	460.921623	9.450240
7.356363	460.349519	9.455258
7.363047	462.155691	9.460275
7.205270	473.004245	9.465293
7.674630	481.779113	9.470311
7.668709	481.636407	9.475328
7.462682	506.589773	9.480346
7.794958	493.130495	9.485363
7.616681	486.562029	9.490381
7.750944	494.072779	9.495399
7.685740	476.276885	9.500416
7.230042	468.756651	9.505434
7.161834	484.854053	9.510451
7.139249	495.928949	9.515469
7.550393	494.682697	9.520487
7.743875	489.006234	9.525504
7.562037	502.504976	9.530522
7.923119	487.815315	9.535539
7.873689	498.423883	9.540557
7.759984	496.390928	9.545575
7.951392	499.916306	9.550592
8.072445	502.565901	9.555610
8.133163	497.129341	9.560627
8.234518	478.280055	9.565645
7.776284	465.032425	9.570663
7.639374	469.456558	9.575680
7.307695	473.032948	9.580698
7.595475	454.596587	9.585715
7.497168	468.461138	9.590733
7.594171	474.382706	9.595751
7.888475	484.332522	9.600768
7.581667	500.294014	9.605786
8.005060	502.177654	9.610803
7.800058	483.481428	9.615821
7.572965	479.440085	9.620839
7.957539	484.968144	9.625856
7.868780	482.451446	9.630874
7.809085	487.883079	9.635891
7.681563	466.283345	9.640909
7.956424	487.195358	9.645927
7.962185	477.964069	9.650944
7.759533	472.927659	9.655962
7.885989	467.390010	9.660979
7.716812	480.201353	9.665997
7.492758	483.036491	9.671015
7.781705	481.330516	9.676032
7.805023	508.961845	9.681050
7.670965	491.524583	9.686067
7.653774	496.339678	9.691085
7.709692	507.742482	9.696103
7.727268	505.804539	9.701120
7.857406	496.921012	9.706138
7.553039	504.080818	9.711155
7.678532	498.407519	9.716173
7.747025	491.396584	9.721191
7.939989	502.450329	9.726208
7.790455	509.099516	9.731226
7.935425	499.110718	9.736243
7.657567	502.462321	9.741261
7.544197	509.489702	9.746279
7.984738	511.543406	9.751296
7.973388	527.918109	9.756314
8.270703	533.945446	9.761331
8.053290	507.900615	9.766349
7.823436	505.491365	9.771367
7.955016	509.412083	9.776384
7.925982	523.240733	9.781402
7.925841	532.518425	9.786419
8.262134	531.790437	9.791437
8.076862	523.382650	9.796455
7.950490	522.363482	9.801472
7.911358	527.574553	9.806490
8.178854	529.667484	9.811507
8.315140	518.486559	9.816525
8.058526	506.870086	9.821543
8.062976	490.694507	9.826560
8.053917	502.322173	9.831578
7.727270	500.186444	9.836595
7.961994	506.648631	9.841613
7.901020	523.904181	9.846631
8.036029	530.601216	9.851648
7.911743	526.741943	9.856666
8.325548	524.019475	9.861683
8.664639	527.982267	9.866701
8.373898	529.802960	9.871719
8.265237	510.560674	9.876736
8.099750	510.446109	9.881754
7.855804	509.614545	9.886771
8.030648	515.594018	9.891789
8.260049	521.510650	9.896807
8.171633	525.172710	9.901824
8.479312	544.836923	9.906842
8.029481	525.873296	9.911859
8.429777	524.483785	9.916877
8.263699	531.961330	9.921895
8.610950	499.322984	9.926912
7.970350	508.847712	9.931930
8.001578	504.721260	9.936947
8.062939	503.094420	9.941965
8.145601	522.772862	9.946983
8.227296	531.795446	9.952000
8.312018	528.898767	9.957018
8.484611	535.100718	9.962035
8.235909	529.036486	9.967053
8.188745	536.528823	9.972071
8.120779	530.254151	9.977088
8.015926	541.916866	9.982106
8.251596	548.860113	9.987123
8.159829	533.361177	9.992141
8.052096	536.631436	9.997159
8.250598	528.771023	10.002176
8.130031	533.945957	10.007194
8.029528	525.624435	10.012211
8.355200	531.101628	10.017229
8.095296	530.211689	10.022247
8.244126	529.044405	10.027264
8.105517	528.388109	10.032282
8.289089	530.073738	10.037299
8.334233	531.013998	10.042317
8.234398	540.176209	10.047335
8.335865	547.626867	10.052352
8.448731	559.491460	10.057370
8.188380	554.494375	10.062387
8.548448	563.030023	10.067405
8.503392	557.761974	10.072423
8.506106	549.319564	10.077440
8.683500	565.468373	10.082458
8.246113	556.032474	10.087475
8.658982	549.307739	10.092493
8.376327	552.271152	10.097511
8.292932	550.238691	10.102528
8.503171	557.443572	10.107546
8.063780	558.060840	10.112563
8.451881	553.463674	10.117581
8.210181	561.666279	10.122599
8.474323	547.794974	10.127616
8.444108	552.887969	10.132634
8.230748	558.972254	10.137651
8.648611	547.232972	10.142669
8.322193	554.953319	10.147687
8.183225	568.235038	10.152704
8.189796	560.965659	10.157722
8.369452	559.654725	10.162739
8.683577	553.607883	10.167757
8.302302	567.585610	10.172775
8.764327	572.489907	10.177792
8.585869	567.470329	10.182810
8.390486	581.717288	10.187827
9.009523	575.475491	10.192845
8.716878	561.682704	10.197863
8.389649	563.296680	10.202880
8.599322	565.938923	10.207898
8.718711	571.109936	10.212915
8.931631	558.626131	10.217933
8.356676	568.188463	10.222951
8.715211	564.059076	10.227968
8.877117	566.681856	10.232986
8.675653	561.757205	10.238003
8.967396	560.282108	10.243021
8.712937	559.432696	10.248039
8.703604	555.529621	10.253056
8.719844	555.933335	10.258074
8.389954	562.855016	10.263091
8.822480	564.937409	10.268109
8.564173	562.582546	10.273127
8.590151	575.658901	10.278144
9.036708	589.330981	10.283162
8.811203	582.880689	10.288179
8.540947	564.506403	10.293197
8.598171	577.120603	10.298215
8.758256	584.096431	10.303232
8.657724	583.790558	10.308250
8.479829	589.717647	10.313267
8.442318	595.661392	10.318285
8.918146	596.236351	10.323303
8.648384	594.972523	10.328320
9.060158	599.794797	10.333338
8.749489	602.468224	10.338355
9.019247	583.914633	10.343373
8.806104	589.669434	10.348391
8.808180	601.648708	10.353408
9.313327	594.158661	10.358426
8.993585	593.356642	10.363443
9.063355	588.875740	10.368461
8.889834	597.743729	10.373479
9.060492	588.699745	10.378496
9.111675	597.392440	10.383514
8.876995	596.233225	10.388531
8.925681	587.022330	10.393549
8.855942	591.725003	10.398567
8.474862	596.796386	10.403584
8.970276	590.019320	10.408602
8.524463	584.101200	10.413619
8.719781	588.400596	10.418637
8.738052	595.615077	10.423655
8.675157	595.050476	10.428672
9.115344	594.135666	10.433690
8.825557	594.828980	10.438707
9.306473	581.637324	10.443725
9.153163	585.076509	10.448743
8.689565	597.174065	10.453760
9.254292	582.648651	10.458778
8.932527	592.884855	10.463795
9.374024	587.436410	10.468813
9.044781	584.127127	10.473831
9.157100	591.079855	10.478848
9.498437	587.496991	10.483866
9.154463	581.632008	10.488883
9.130468	590.056767	10.493901
9.044987	585.124455	10.498919
9.086821	600.648002	10.503936
9.221665	590.694374	10.508954
9.176711	591.969048	10.513971
9.179340	589.076575	10.518989
8.972322	579.809536	10.524007
9.043838	593.095560	10.529024
8.851453	590.680105	10.534042
8.663612	582.974239	10.539059
8.929719	578.244108	10.544077
9.214486	599.779017	10.549095
9.413393	599.279889	10.554112
9.391493	586.353077	10.559130
8.821810	584.416915	10.564147
9.305777	594.029223	10.569165
9.079230	587.882681	10.574183
8.771699	609.720462	10.579200
9.130347	614.349691	10.584218
9.162864	613.691582	10.589235
9.279785	614.629433	10.594253
9.416611	619.214334	10.599271
9.468661	619.896227	10.604288
9.708690	610.032958	10.609306
9.599902	615.219454	10.614323
9.393695	588.776454	10.619341
9.315313	589.990918	10.624359
8.897585	588.718086	10.629376
9.474610	590.641197	10.634394
9.325443	608.533140	10.639411
9.455137	618.502373	10.644429
9.090108	610.732487	10.649447
9.488071	616.071313	10.654464
9.505490	615.965292	10.659482
9.115432	625.707887	10.664499
9.089374	608.237195	10.669517
9.341755	613.143479	10.674535
9.353729	621.606200	10.679552
9.552863	615.023429	10.684570
9.369489	619.044540	10.689587
9.887734	617.226558	10.694605
9.621878	614.507163	10.699623
9.752877	612.931388	10.704640
9.563738	596.985778	10.709658
8.966951	592.424615	10.714675
9.427199	591.412611	10.719693
9.671506	614.613435	10.724711
9.367759	626.251614	10.729728
9.661389	610.756908	10.734746
9.442913	616.937120	10.739763
9.662677	611.626372	10.744781
9.475969	615.596763	10.749799
9.103839	616.354758	10.754816
9.578597	609.942244	10.759834
9.640882	620.949475	10.764851
9.479794	623.416137	10.769869
9.762761	627.905546	10.774887
9.676683	621.006496	10.779904
9.912211	611.265598	10.784922
9.486239	607.810320	10.789939
9.502915	602.451263	10.794957
9.673332	595.368921	10.799975
9.611357	614.458123	10.804992
9.547737	609.888651	10.810010
9.463034	626.421713	10.815027
9.647058	619.132330	10.820045
9.692448	616.829416	10.825063
9.460261	621.777895	10.830080
9.814287	620.656009	10.835098
9.693902	615.986883	10.840115
9.313835	622.389824	10.845133
9.673982	623.155913	10.850151
9.404570	620.722775	10.855168
9.877743	616.713280	10.860186
9.607938	618.063787	10.865203
9.512368	616.298532	10.870221
9.975289	618.894800	10.875239
9.463927	617.568850	10.880256
9.835593	616.190952	10.885274
9.572119	625.489289	10.890291
9.626797	614.216290	10.895309
9.933558	619.012036	10.900327
9.726822	622.711779	10.905344
9.690863	615.777978	10.910362
9.759501	619.390785	10.915379
9.538803	621.602390	10.920397
9.703681	620.360612	10.925415
9.460369	641.209285	10.930432
10.286787	649.247330	10.935450
10.100161	646.076539	10.940467
9.684380	635.153559	10.945485
10.029379	627.617437	10.950503
9.384481	628.658059	10.955520
9.678241	641.350227	10.960538
10.019785	652.763110	10.965555
9.789195	654.016313	10.970573
10.068165	655.633543	10.975591
9.941287	663.671193	10.980608
10.242970	650.328327	10.985626
9.976787	651.292785	10.990643
9.848601	654.296327	10.995661
10.139402	648.830252	11.000679
9.871333	657.437480	11.005696
10.296222	657.381618	11.010714
10.140483	639.305084	11.015731
9.623390	632.629588	11.020749
10.109271	650.189711	11.025767
10.009633	652.035223	11.030784
10.170832	648.076685	11.035802
10.265229	662.731939	11.040819
9.876848	643.460826	11.045837
9.940709	634.220137	11.050855
9.945491	645.287174	11.055872
10.112443	660.358302	11.060890
10.178446	647.552514	11.065907
9.874252	653.806934	11.070925
10.236654	658.493418	11.075943
10.134281	660.338301	11.080960
10.091470	652.304164	11.085978
10.200996	651.373537	11.090995
9.855699	659.309020	11.096013
10.419213	653.325727	11.101031
10.002923	652.102445	11.106048
9.984733	659.705582	11.111066
10.355594	646.472916	11.116083
9.839453	641.862393	11.121101
10.187785	648.731665	11.126119
10.196223	648.837715	11.131136
10.046903	636.024813	11.136154
10.303561	642.107228	11.141171
9.944804	654.810606	11.146189
10.144446	641.717240	11.151207
10.199918	651.566701	11.156224
10.219320	647.818073	11.161242
10.403724	644.737610	11.166259
10.069683	651.246615	11.171277
10.042567	646.541303	11.176295
10.011847	658.140291	11.181312
10.256777	651.376055	11.186330
10.539381	638.558392	11.191347
10.207101	657.067541	11.196365
10.349217	647.579313	11.201383
10.524116	649.652433	11.206400
10.623380	652.150469	11.211418
10.285167	641.061154	11.216435
10.171597	642.648882	11.221453
10.502544	643.648491	11.226471
10.427382	647.317936	11.231488
10.475136	643.666376	11.236506
10.273861	648.977299	11.241523
10.213514	654.756371	11.246541
10.710485	663.488207	11.251559
10.549024	665.242973	11.256576
10.247623	658.334125	11.261594
10.184656	653.095376	11.266611
10.529110	677.002629	11.271629
10.664595	670.226851	11.276647
10.645816	672.343395	11.281664
10.628108	665.503288	11.286682
10.489363	658.671377	11.291699
10.197428	654.324724	11.296717
10.626767	659.008806	11.301735
10.598240	676.214489	11.306752
10.769011	671.466332	11.311770
10.888941	675.182759	11.316787
10.479859	669.732850	11.321805
10.757862	660.059789	11.326823
10.619342	656.396202	11.331840
10.228973	653.849216	11.336858
10.698545	656.894399	11.341875
10.629809	672.832078	11.346893
10.852471	673.657399	11.351911
10.419002	658.595339	11.356928
10.549481	664.506331	11.361946
11.004418	672.824632	11.366963
10.402998	668.896859	11.371981
10.740793	663.030179	11.376999
10.833861	680.975267	11.382016
10.671891	676.802956	11.387034
10.546089	666.625673	11.392051
10.575304	689.149994	11.397069
10.801780	678.454933	11.402087
10.595366	685.492752	11.407104
10.877943	677.181842	11.412122
10.873208	675.879130	11.417139
10.717289	677.846916	11.422157
10.657550	679.834922	11.427175
10.884530	684.961034	11.432192
10.618117	674.791140	11.437210
10.713339	680.223908	11.442227
10.567527	683.782817	11.447245
10.846743	680.243754	11.452263
10.567276	681.879863	11.457280
10.598862	692.201313	11.462298
10.953421	681.345348	11.467315
10.965508	676.879955	11.472333
11.024772	673.010978	11.477351
10.673339	677.165564	11.482368
10.307324	673.757044	11.487386
10.822908	676.293645	11.492403
10.758006	683.870858	11.497421
11.068495	670.582906	11.502439
10.793836	680.241714	11.507456
10.489036	678.483573	11.512474
10.807038	703.562920	11.517491
10.732575	706.810791	11.522509
10.947913	706.933723	11.527527
11.055304	715.615523	11.532544
10.787475	711.737216	11.537562
11.084768	713.339912	11.542579
10.987656	721.244647	11.547597
11.101828	717.101086	11.552615
11.255352	707.870038	11.557632
11.225659	726.203896	11.562650
11.225228	714.553393	11.567667
10.783015	718.797879	11.572685
11.135440	708.944707	11.577703
11.274067	713.992731	11.582720
11.256283	716.195616	11.587738
11.405569	709.878079	11.592755
11.267135	712.141345	11.597773
11.151717	711.106774	11.602791
11.313501	715.511630	11.607808
10.598456	703.869113	11.612826
11.010044	709.937466	11.617843
11.007292	720.301217	11.622861
11.129939	709.694932	11.627879
10.960624	707.403574	11.632896
11.026302	718.372723	11.637914
10.858877	709.707998	11.642931
11.024668	716.652143	11.647949
10.981376	714.132026	11.652967
11.006637	709.159428	11.657984
10.805280	727.350726	11.663002
11.125031	737.344030	11.668019
11.153049	742.547029	11.673037
11.323049	739.605809	11.678055
11.469674	753.583457	11.683072
11.069165	737.056217	11.688090
11.311696	739.032559	11.693107
11.202593	752.666912	11.698125
11.378493	746.846734	11.703143
11.407916	738.757316	11.708160
11.391505	754.827448	11.713178
11.522195	747.662249	11.718195
11.467647	749.439605	11.723213
11.209284	750.991048	11.728231
11.372599	747.335520	11.733248
11.262749	742.967311	11.738266
11.624084	737.474395	11.743283
11.602000	749.383086	11.748301
11.301610	748.593113	11.753319
11.652770	743.527777	11.758336
11.369975	747.015951	11.763354
11.737952	733.373826	11.768371
11.555532	734.352001	11.773389
11.341491	746.246062	11.778407
11.694340	740.535594	11.783424
11.517645	746.234735	11.788442
11.644710	753.812339	11.793459
11.336211	743.623375	11.798477
11.259011	751.974747	11.803495
11.622499	745.133408	11.808512
11.265954	744.275467	11.813530
11.229639	747.129815	11.818547
11.333944	749.643960	11.823565
11.351555	744.463896	11.828583
11.492278	752.394390	11.833600
11.498497	759.689763	11.838618
11.815422	754.512880	11.843635
12.136033	762.247640	11.848653
11.979782	767.587475	11.853671
11.811737	754.121101	11.858688
11.533252	753.947466	11.863706
11.531977	747.084828	11.868723
11.891297	741.776065	11.873741
11.627802	750.782412	11.878759
11.654966	747.392841	11.883776
11.554574	739.217416	11.888794
11.779190	741.867847	11.893811
11.623464	748.326367	11.898829
11.790022	745.497701	11.903847
11.837866	744.899246	11.908864
11.651312	752.141155	11.913882
11.689056	761.742975	11.918899
11.939797	782.534795	11.923917
12.067784	776.915105	11.928935
11.970177	751.126583	11.933952
11.621709	766.732019	11.938970
11.855779	772.598675	11.943987
12.113424	775.594964	11.949005
11.884775	764.016285	11.954023
12.000164	743.997258	11.959040
11.612249	743.786501	11.964058
12.099620	756.545175	11.969075
12.073528	759.855818	11.974093
11.743696	748.820049	11.979111
12.034879	750.434780	11.984128
11.841399	764.024830	11.989146
11.989936	764.900784	11.994163
12.168101	767.130731	11.999181
11.850238	772.722527	12.004199
12.169571	764.853145	12.009216
11.943571	775.731588	12.014234
12.125797	786.478810	12.019251
11.973959	778.116529	12.024269
12.206114	775.085028	12.029287
12.357157	772.802911	12.034304
11.675369	753.500044	12.039322
11.976811	759.981916	12.044339
12.293397	774.134606	12.049357
12.055318	773.015892	12.054375
12.111151	776.259073	12.059392
11.997580	783.588227	12.064410
12.082400	771.614105	12.069427
12.225952	779.725016	12.074445
11.945867	779.104487	12.079463
12.021079	776.905262	12.084480
12.055620	780.517345	12.089498
11.884797	770.303052	12.094515
12.091586	776.682191	12.099533
11.821455	785.537125	12.104551
11.812643	783.078313	12.109568
11.802073	773.714138	12.114586
12.219841	792.747504	12.119603
12.411075	797.818845	12.124621
12.317767	806.337641	12.129639
12.254976	808.165864	12.134656
12.509590	815.435960	12.139674
12.379803	793.755347	12.144691
12.227515	774.591482	12.149709
11.821061	789.712524	12.154727
12.312301	800.437522	12.159744
12.452313	804.663950	12.164762
12.497574	810.849760	12.169779
12.562472	812.476700	12.174797
12.074981	817.069870	12.179815
12.815702	814.007555	12.184832
12.506668	812.279817	12.189850
12.615491	810.820756	12.194867
12.746189	795.352593	12.199885
12.140157	791.707190	12.204903
12.242553	773.514625	12.209920
12.457874	795.671011	12.214938
12.719401	800.122388	12.219955
12.119725	794.818672	12.224973
12.218401	811.603858	12.229991
12.216885	807.336898	12.235008
12.623348	808.100460	12.240026
12.800103	804.494459	12.245043
12.622018	806.238999	12.250061
12.206666	805.179986	12.255079
12.432966	793.797899	12.260096
12.406976	803.970801	12.265114
12.518789	813.289795	12.270131
12.907443	806.911800	12.275149
12.466291	807.310414	12.280167
12.682438	799.512387	12.285184
12.734110	806.827726	12.290202
12.378150	807.313424	12.295219
12.574232	807.591871	12.300237
12.561665	803.803714	12.305255
12.546829	798.670522	12.310272
12.540614	802.481927	12.315290
12.558476	796.601938	12.320307
12.678726	813.866834	12.325325
12.663073	834.848882	12.330343
12.513587	834.401909	12.335360
12.989832	834.362653	12.340378
12.866301	849.126231	12.345395
12.910649	831.501157	12.350413
12.941757	833.616072	12.355431
13.070577	830.562865	12.360448
12.940315	823.313219	12.365466
12.739545	804.892326	12.370483
12.783682	806.403133	12.375501
12.399290	815.203555	12.380519
12.857561	821.984967	12.385536
12.836940	826.892350	12.390554
12.927928	833.958633	12.395571
13.029809	833.132684	12.400589
12.967353	833.175760	12.405607
13.010825	835.055901	12.410624
13.042252	829.034019	12.415642
12.861348	834.412001	12.420659
12.908398	834.697463	12.425677
12.904615	836.737057	12.430695
13.274704	837.759340	12.435712
13.145479	837.549524	12.440730
13.029950	839.551691	12.445747
13.039256	840.893586	12.450765
12.896355	842.270474	12.455783
13.130868	826.737791	12.460800
12.972191	841.493787	12.465818
12.728441	835.252171	12.470835
13.078843	824.322889	12.475853
12.561838	833.766675	12.480871
12.871977	840.786215	12.485888
13.017891	831.924982	12.490906
12.912939	839.588206	12.495923
13.369215	832.491777	12.500941
13.265773	842.013160	12.505959
13.244319	829.046510	12.510976
13.324088	837.165237	12.515994
12.973076	837.485975	12.521011
13.206886	819.511358	12.526029
12.981614	833.111447	12.531047
13.039292	833.240654	12.536064
13.330846	830.468763	12.541082
13.021287	842.611809	12.546099
13.107889	853.133291	12.551117
13.037581	866.031254	12.556135
13.481992	862.242649	12.561152
13.622846	863.599414	12.566170
13.395126	867.193943	12.571187
13.606584	870.009829	12.576205
13.271311	857.645995	12.581223
13.358215	859.419571	12.586240
13.773089	852.545879	12.591258
13.249964	854.992598	12.596275
13.521918	840.776988	12.601293
13.149108	837.767707	12.606311
13.191012	858.289573	12.611328
13.498986	861.894277	12.616346
13.265609	864.172272	12.621363
13.332628	854.932798	12.626381
13.189953	873.189261	12.631399
13.580091	867.754519	12.636416
13.722004	864.636849	12.641434
13.564452	878.323800	12.646451
13.806121	862.156355	12.651469
13.577258	864.611917	12.656487
13.659342	870.499693	12.661504
13.773730	873.047225	12.666522
13.477714	858.289554	12.671539
13.647234	868.517870	12.676557
13.459267	869.606299	12.681575
13.358031	866.216763	12.686592
13.905705	869.579139	12.691610
13.726798	866.189252	12.696627
13.637444	859.467374	12.701645
13.761751	863.569666	12.706663
13.406493	868.409551	12.711680
13.671526	865.956347	12.716698
13.526335	873.991819	12.721715
13.887187	857.756661	12.726733
13.685563	869.012566	12.731751
13.455132	871.292535	12.736768
13.551178	866.868615	12.741786
13.032445	872.548848	12.746803
13.379551	865.658008	12.751821
13.734156	886.953771	12.756839
14.284341	886.513098	12.761856
14.074681	889.532314	12.766874
13.670147	881.645120	12.771891
13.590730	864.332041	12.776909
14.083500	894.752383	12.781927
13.999405	892.500545	12.786944
14.027130	874.227798	12.791962
14.115675	871.602321	12.796979
13.921495	859.140085	12.801997
13.637708	858.065033	12.807015
13.918185	867.614506	12.812032
14.218691	879.346388	12.817050
14.083726	871.567281	12.822067
14.310789	869.239719	12.827085
14.142613	877.334985	12.832103
13.481306	869.089420	12.837120
13.867779	859.640685	12.842138
13.820254	875.970073	12.847155
13.772767	890.647319	12.852173
14.104806	896.382599	12.857191
13.787586	899.719635	12.862208
14.116645	883.179525	12.867226
14.079168	892.895020	12.872243
14.117081	900.327814	12.877261
14.281346	894.281101	12.882279
14.105805	903.331357	12.887296
14.251913	892.900465	12.892314
14.106544	901.204632	12.897331
14.334495	898.168585	12.902349
14.312562	895.496314	12.907367
14.126699	892.757549	12.912384
14.523662	892.612815	12.917402
14.179642	902.748197	12.922419
14.351762	891.176899	12.927437
14.383624	897.891042	12.932455
14.171310	903.974501	12.937472
14.384374	895.111287	12.942490
14.306673	889.867609	12.947507
14.134169	892.401837	12.952525
14.434372	890.880439	12.957543
14.495383	890.107394	12.962560
14.344666	893.118346	12.967578
14.471784	895.514888	12.972595
14.285657	893.176781	12.977613
14.734501	893.518657	12.982631
14.332024	905.794900	12.987648
14.328090	895.305451	12.992666
14.218455	902.727793	12.997683
14.330915	897.672627	13.002701
14.475821	890.977858	13.007719
14.268182	899.227562	13.012736
14.459432	894.711046	13.017754
14.171383	896.903905	13.022771
14.045262	891.670196	13.027789
14.477549	884.887492	13.032807
14.418550	888.622716	13.037824
14.485972	902.054538	13.042842
14.115983	906.248662	13.047859
14.381166	916.965340	13.052877
14.436518	916.473492	13.057895
14.380503	922.065566	13.062912
14.665708	919.350013	13.067930
14.739539	919.244508	13.072947
14.943861	918.204516	13.077965
14.798043	916.661860	13.082983
14.823905	921.305142	13.088000
14.941382	918.217282	13.093018
14.936975	918.969433	13.098035
14.804965	922.021976	13.103053
14.626184	919.714534	13.108071
14.664069	924.638948	13.113088
15.027457	912.537397	13.118106
15.082762	922.004058	13.123123
14.797285	916.789787	13.128141
15.052479	906.284373	13.133159
14.803022	911.874657	13.138176
15.047659	904.927223	13.143194
14.757285	887.996159	13.148211
14.860539	889.555264	13.153229
14.933898	891.440609	13.158247
14.674781	900.823809	13.163264
15.017191	904.561390	13.168282
15.076346	912.978685	13.173299
15.052249	911.033013	13.178317
15.127265	904.029767	13.183335
14.663848	900.201448	13.188352
14.601469	902.360459	13.193370
15.012726	904.798022	13.198387
14.959221	916.156232	13.203405
15.117278	910.585451	13.208423
15.037018	901.245606	13.213440
15.119037	909.784788	13.218458
14.988264	919.253659	13.223475
14.909604	907.490174	13.228493
15.174088	918.310098	13.233511
15.031985	912.415071	13.238528
15.318244	908.421727	13.243546
15.187511	909.218765	13.248563
14.693636	913.267548	13.253581
15.009340	904.845549	13.258599
15.030630	899.194637	13.263616
14.867113	907.884904	13.268634
14.943944	915.991463	13.273651
14.733672	911.962872	13.278669
15.158054	923.538220	13.283687
15.077006	943.777622	13.288704
15.509146	936.901039	13.293722
15.386036	944.646239	13.298739
15.627718	944.409077	13.303757
15.488179	939.093137	13.308775
15.070645	926.979412	13.313792
15.793984	921.887743	13.318810
15.268082	912.585913	13.323827
15.230141	918.541270	13.328845
15.352677	927.561865	13.333863
15.283527	941.893788	13.338880
15.737824	945.140238	13.343898
15.881426	933.087391	13.348915
15.400771	921.568542	13.353933
15.675592	920.235258	13.358951
15.708988	927.496796	13.363968
15.200932	912.524947	13.368986
15.256459	911.131170	13.374003
15.122539	913.248569	13.379021
15.779150	928.890104	13.384039
15.576858	942.111068	13.389056
15.595283	941.757384	13.394074
15.724207	943.332623	13.399091
15.499011	926.195506	13.404109
15.762980	942.899395	13.409127
15.522748	939.933822	13.414144
15.875812	931.677454	13.419162
15.400793	927.883027	13.424179
15.743265	939.503414	13.429197
15.824690	940.011896	13.434215
15.584672	944.694203	13.439232
15.863635	938.679886	13.444250
15.814816	939.110008	13.449267
15.759078	934.076230	13.454285
15.625195	918.596953	13.459303
15.398913	935.317296	13.464320
15.491118	945.963779	13.469338
15.583266	935.327838	13.474355
15.460465	944.198469	13.479373
15.545029	947.285982	13.484391
15.588155	940.442982	13.489408
15.595449	940.370023	13.494426
15.935204	947.176194	13.499443
15.508565	946.303943	13.504461
15.890159	951.589992	13.509479
16.296666	970.797162	13.514496
16.136778	952.938622	13.519514
16.362480	936.728962	13.524531
15.976733	946.295980	13.529549
16.178534	934.087872	13.534567
15.831330	951.274787	13.539584
15.964996	954.276248	13.544602
15.844625	945.113939	13.549619
15.649119	939.441959	13.554637
16.253792	947.668945	13.559655
15.992872	957.867487	13.564672
15.928238	950.364755	13.569690
16.080267	969.238159	13.574707
16.158587	976.046805	13.579725
16.288474	971.379610	13.584743
16.287918	972.994947	13.589760
16.318083	973.989079	13.594778
16.317873	942.547757	13.599795
15.779400	936.664492	13.604813
15.915771	955.979560	13.609831
16.137346	976.003178	13.614848
16.290751	966.319714	13.619866
16.581713	966.047839	13.624883
16.166302	979.417321	13.629901
16.114529	969.013961	13.634919
16.131824	981.534323	13.639936
16.035347	979.224391	13.644954
16.368011	974.131531	13.649971
16.279669	977.992666	13.654989
16.360883	972.124775	13.660007
16.388406	971.700210	13.665024
16.191037	979.054917	13.670042
16.399430	977.590702	13.675059
16.122154	990.883439	13.680077
16.564496	969.191973	13.685095
16.561130	976.659475	13.690112
16.321950	981.663644	13.695130
16.362028	972.422253	13.700147
16.169791	981.570278	13.705165
16.312711	980.438774	13.710183
16.590075	1003.481600	13.715200
16.401638	1012.133828	13.720218
16.679207	1009.829094	13.725235
16.647200	1001.050896	13.730253
16.856024	1008.662942	13.735271
16.786994	1012.286586	13.740288
16.673911	1006.432093	13.745306
16.746053	993.897690	13.750323
16.773771	1005.296568	13.755341
17.045758	990.082667	13.760359
16.889935	981.212560	13.765376
16.694168	977.847970	13.770394
16.747593	961.618928	13.775411
16.686314	984.116419	13.780429
16.889437	980.112882	13.785447
16.915014	973.866853	13.790464
16.645416	973.132693	13.795482
16.684483	966.379706	13.800499
16.922456	980.057280	13.805517
16.869173	972.100283	13.810535
17.087206	967.672216	13.815552
16.892506	974.013572	13.820570
16.959405	974.843394	13.825587
16.580028	973.799187	13.830605
16.713813	961.472399	13.835623
16.966454	985.457992	13.840640
16.756877	982.605828	13.845658
17.172494	988.171748	13.850675
16.969685	1000.898350	13.855693
17.154787	1001.077749	13.860711
16.997298	992.977951	13.865728
16.867323	997.249540	13.870746
17.209258	996.132087	13.875763
17.113629	1007.685186	13.880781
17.069817	999.889375	13.885799
17.053058	999.901972	13.890816
16.878868	997.333176	13.895834
17.024334	1003.346725	13.900851
17.154812	1005.121285	13.905869
17.297757	1003.156164	13.910887
17.267801	1006.259760	13.915904
17.237555	1005.816104	13.920922
17.440656	1001.050595	13.925939
16.915395	1009.747954	13.930957
17.126781	1012.201737	13.935975
17.197577	1003.618815	13.940992
17.155312	1013.573619	13.946010
17.264476	1004.266373	13.951027
17.150922	1008.692508	13.956045
17.283662	1010.867411	13.961063
17.227494	1007.441267	13.966080
17.093790	1011.143008	13.971098
17.316719	1004.558895	13.976115
16.983458	999.341766	13.981133
16.980643	1005.495350	13.986151
17.152347	1005.243084	13.991168
17.578545	1020.613297	13.996186
17.670375	1027.365117	14.001203
17.610283	1025.259758	14.006221
17.489628	1025.455144	14.011239
17.795050	1024.486906	14.016256
17.463739	1033.535623	14.021274
17.540146	1019.322937	14.026291
17.671192	1030.762229	14.031309
17.725829	1032.471682	14.036327
17.787575	1024.845094	14.041344
17.490184	1007.694919	14.046362
17.598908	1025.207878	14.051379
17.891488	1021.849372	14.056397
17.641957	1010.642888	14.061415
17.602933	1001.812316	14.066432
17.278161	1009.723822	14.071450
17.948525	1007.410270	14.076467
18.139679	1023.616824	14.081485
17.724624	1025.276555	14.086503
17.698037	1009.084894	14.091520
17.748837	1011.823929	14.096538
17.793440	1020.284330	14.101555
17.702445	1019.871575	14.106573
17.864084	1029.449447	14.111591
18.080471	1023.530955	14.116608
17.823428	1032.155956	14.121626
18.256930	1030.562525	14.126643
17.975603	1023.835200	14.131661
17.686367	1006.767817	14.136679
18.160055	1016.365557	14.141696
17.873242	1029.432089	14.146714
17.655560	1017.968511	14.151731
17.744832	1015.998580	14.156749
17.938467	1024.457875	14.161767
17.987652	1017.524386	14.166784
17.709673	1023.267921	14.171802
17.706817	1019.916512	14.176819
17.853870	1022.091807	14.181837
17.812499	1013.946435	14.186855
17.972352	1017.938090	14.191872
17.997549	1020.878861	14.196890
18.173970	1003.912745	14.201907
18.182842	1021.382074	14.206925
18.088625	1034.622850	14.211943
18.198494	1016.115335	14.216960
17.786395	1029.244591	14.221978
18.218209	1042.646530	14.226995
17.813294	1043.613370	14.232013
17.966572	1054.537777	14.237031
18.462761	1049.976531	14.242048
18.423063	1035.150845	14.247066
18.665730	1042.039134	14.252083
18.360827	1053.650862	14.257101
18.355236	1056.514951	14.262119
18.440200	1046.082251	14.267136
18.359944	1044.707555	14.272154
18.181543	1047.241405	14.277171
18.366408	1043.474588	14.282189
18.311132	1048.583600	14.287207
18.582612	1046.101552	14.292224
18.616721	1040.961666	14.297242
18.538817	1046.706490	14.302259
18.770484	1049.371654	14.307277
18.461440	1052.426515	14.312295
18.436174	1043.163013	14.317312
18.296812	1047.781973	14.322330
18.073238	1039.025177	14.327347
18.348330	1049.088554	14.332365
18.174527	1055.180667	14.337383
19.043089	1058.113254	14.342400
18.510359	1070.943835	14.347418
18.712882	1069.287703	14.352435
18.815196	1064.780028	14.357453
18.880843	1071.973816	14.362471
19.053913	1047.807196	14.367488
18.947108	1056.358966	14.372506
18.702043	1055.286456	14.377523
18.758737	1052.603722	14.382541
18.273176	1050.897058	14.387559
18.577340	1053.591278	14.392576
18.901955	1074.096432	14.397594
19.168299	1088.487400	14.402611
19.201500	1073.560767	14.407629
19.035711	1066.072924	14.412647
18.561692	1043.369014	14.417664
18.475474	1054.216090	14.422682
18.701472	1070.094747	14.427699
18.787592	1071.784536	14.432717
19.010332	1075.536916	14.437735
19.670857	1071.237235	14.442752
19.375316	1081.419143	14.447770
19.349302	1061.965200	14.452787
18.941468	1046.621404	14.457805
19.268793	1060.788428	14.462823
19.140021	1044.577402	14.467840
19.160275	1042.409067	14.472858
18.883728	1051.400918	14.477875
19.305664	1041.183255	14.482893
19.268830	1044.342514	14.487911
19.053140	1034.323320	14.492928
18.739803	1045.316762	14.497946
19.274662	1061.105400	14.502963
19.422844	1066.357929	14.507981
19.086111	1064.001384	14.512999
19.493376	1061.341410	14.518016
19.428484	1067.943588	14.523034
19.646198	1065.278920	14.528051
19.276341	1040.073884	14.533069
18.810043	1041.072321	14.538087
19.237213	1051.946052	14.543104
19.401086	1062.925889	14.548122
19.455353	1067.109187	14.553139
19.671979	1062.425367	14.558157
19.563528	1070.759935	14.563175
19.866506	1058.988078	14.568192
19.773954	1066.356406	14.573210
19.676934	1048.280019	14.578227
19.643100	1036.847845	14.583245
19.748750	1040.044274	14.588263
19.483115	1035.052234	14.593280
19.627813	1031.868531	14.598298
19.743359	1033.466656	14.603315
19.842766	1032.405714	14.608333
19.656828	1028.336955	14.613351
19.837102	1031.211557	14.618368
19.591630	1036.812151	14.623386
19.673647	1034.512962	14.628403
19.589574	1026.483283	14.633421
19.663647	1033.667689	14.638439
19.624133	1029.885405	14.643456
19.739559	1036.448324	14.648474
19.636922	1038.684269	14.653491
19.565641	1035.351250	14.658509
19.509272	1046.898678	14.663527
19.700306	1069.190650	14.668544
19.927258	1072.782814	14.673562
19.692621	1062.924481	14.678579
19.906382	1065.611796	14.683597
19.733330	1075.507362	14.688615
20.005973	1068.873183	14.693632
20.073859	1062.310731	14.698650
20.022932	1070.556771	14.703667
20.206088	1071.776272	14.708685
19.931359	1076.257501	14.713703
20.422133	1069.862227	14.718720
20.077134	1069.662971	14.723738
19.882691	1064.446398	14.728755
19.973662	1069.949089	14.733773
19.949629	1071.733741	14.738791
19.962210	1068.593414	14.743808
19.896782	1069.786782	14.748826
19.859176	1064.548228	14.753843
20.393058	1056.626415	14.758861
20.061372	1063.843151	14.763879
19.743397	1067.669927	14.768896
19.732195	1064.683801	14.773914
20.220556	1090.170984	14.778931
20.280685	1091.534025	14.783949
20.031125	1099.182108	14.788967
20.414206	1084.848025	14.793984
20.635799	1104.375929	14.799002
20.332251	1097.184903	14.804019
20.685990	1090.949938	14.809037
20.706910	1098.139222	14.814055
20.661398	1108.386109	14.819072
20.503534	1076.610195	14.824090
20.173511	1064.403173	14.829107
20.339611	1085.405223	14.834125
20.440381	1086.586971	14.839143
20.533760	1084.614679	14.844160
20.658766	1095.800436	14.849178
20.403869	1103.560507	14.854195
20.559335	1095.066280	14.859213
20.584172	1101.263553	14.864231
20.352549	1094.172041	14.869248
20.703205	1084.157139	14.874266
20.480426	1095.241932	14.879283
20.482647	1093.446979	14.884301
20.280192	1092.235656	14.889319
20.459655	1105.429100	14.894336
20.387004	1095.559230	14.899354
20.359296	1096.054163	14.904371
20.658363	1092.444121	14.909389
20.618977	1118.126517	14.914407
20.835439	1113.535508	14.919424
21.050271	1111.890720	14.924442
20.743628	1126.770833	14.929459
21.178367	1111.354061	14.934477
21.095687	1117.954869	14.939495
20.873322	1116.132766	14.944512
20.940743	1105.968922	14.949530
21.341091	1116.506344	14.954547
21.128119	1099.175609	14.959565
21.061416	1086.193192	14.964583
21.063684	1084.327771	14.969600
20.904294	1076.072069	14.974618
20.736841	1094.067384	14.979635
21.209913	1104.290567	14.984653
21.321185	1111.249904	14.989671
21.380732	1110.464296	14.994688
21.696134	1086.093418	14.999706
21.084245	1089.838183	15.004723
21.476877	1087.029074	15.009741
21.065985	1087.314443	15.014759
20.834158	1078.778143	15.019776
21.219249	1082.292413	15.024794
21.410024	1086.320603	15.029811
21.196473	1077.361277	15.034829
20.946262	1091.257692	15.039847
21.244206	1101.150624	15.044864
21.444849	1100.273897	15.049882
21.484207	1106.956287	15.054899
21.483992	1101.515414	15.059917
21.701428	1106.133490	15.064935
21.536380	1090.981870	15.069952
21.436857	1087.061483	15.074970
21.270690	1072.011722	15.079987
21.605406	1091.413257	15.085005
21.391712	1090.324637	15.090023
21.380115	1104.044647	15.095040
21.489360	1100.518718	15.100058
21.330953	1109.112799	15.105075
21.683437	1103.985721	15.110093
21.603020	1098.546785	15.115111
21.372595	1111.804920	15.120128
21.610976	1099.199167	15.125146
21.494660	1108.125898	15.130163
21.651656	1099.547178	15.135181
21.654165	1106.245991	15.140199
21.262507	1094.770069	15.145216
21.696524	1094.162597	15.150234
21.364444	1102.451081	15.155251
22.013654	1109.408513	15.160269
21.792210	1111.131517	15.165287
21.749220	1112.613846	15.170304
22.018249	1112.577739	15.175322
21.612772	1112.469860	15.180339
21.767917	1127.267756	15.185357
21.928071	1127.619263	15.190375
22.065118	1132.204183	15.195392
22.250978	1131.083974	15.200410
22.104197	1138.804645	15.205427
21.984287	1120.645160	15.210445
22.037791	1122.318398	15.215463
22.148082	1119.601111	15.220480
22.167732	1100.966006	15.225498
21.958133	1106.749149	15.230515
22.180321	1118.840260	15.235533
21.909187	1128.393764	15.240551
22.205672	1126.944107	15.245568
22.653970	1115.866279	15.250586
21.882232	1117.332447	15.255603
22.518090	1121.398984	15.260621
22.585337	1114.211427	15.265639
22.218648	1105.085987	15.270656
22.261321	1103.236521	15.275674
22.209847	1100.031984	15.280691
22.301901	1114.899635	15.285709
22.475753	1121.926672	15.290727
22.160639	1122.846005	15.295744
22.485914	1123.544373	15.300762
22.375088	1139.142995	15.305779
22.190798	1131.933819	15.310797
22.324450	1130.818105	15.315815
22.350337	1139.252832	15.320832
22.179988	1120.331144	15.325850
22.394753	1129.316049	15.330867
22.148663	1130.426107	15.335885
22.191541	1134.008455	15.340903
22.244314	1127.698922	15.345920
22.543615	1148.776275	15.350938
22.278484	1163.427160	15.355955
22.481611	1157.194720	15.360973
22.851343	1158.628925	15.365991
22.661276	1164.638350	15.371008
23.163376	1148.749659	15.376026
22.826381	1167.351522	15.381043
23.115024	1157.853724	15.386061
22.998216	1149.184026	15.391079
22.677639	1151.521544	15.396096
22.911121	1147.299303	15.401114
22.784116	1147.064119	15.406131
22.928389	1150.269737	15.411149
23.379826	1149.428617	15.416167
22.572522	1132.695876	15.421184
23.028246	1133.809621	15.426202
23.249864	1157.928443	15.431219
23.055121	1139.605938	15.436237
23.015166	1135.851452	15.441255
22.802115	1141.121683	15.446272
23.043004	1146.726279	15.451290
23.087069	1156.802221	15.456307
22.869662	1162.134979	15.461325
23.196505	1152.167564	15.466343
23.158300	1158.519349	15.471360
23.258426	1162.432343	15.476378
23.217876	1161.972475	15.481395
23.393315	1153.997661	15.486413
23.367253	1154.229770	15.491431
23.437221	1150.734431	15.496448
23.577474	1143.764284	15.501466
23.047115	1139.426975	15.506483
23.222605	1156.889984	15.511501
23.446298	1152.349334	15.516519
23.201396	1155.486020	15.521536
23.436910	1148.982134	15.526554
23.483607	1157.622452	15.531571
23.177094	1152.523663	15.536589
23.462979	1152.148410	15.541607
23.062472	1157.900335	15.546624
23.524007	1157.069551	15.551642
23.993563	1161.788673	15.556659
23.686240	1154.248302	15.561677
23.551603	1152.658113	15.566695
23.548838	1160.331180	15.571712
23.764311	1146.877644	15.576730
23.398446	1154.519980	15.581747
23.176244	1156.432255	15.586765
23.773110	1156.913528	15.591783
23.462291	1145.101232	15.596800
23.328416	1141.719685	15.601818
23.703890	1148.809463	15.606835
23.464644	1149.276374	15.611853
23.421864	1155.702917	15.616871
23.780387	1176.037967	15.621888
23.755149	1179.327500	15.626906
23.771879	1176.918135	15.631923
24.057543	1185.809087	15.636941
23.847197	1174.220873	15.641959
23.819068	1180.934326	15.646976
24.262500	1187.920585	15.651994
24.116584	1178.860864	15.657011
23.970848	1180.530820	15.662029
24.088157	1183.448233	15.667047
24.099306	1188.379511	15.672064
24.023355	1175.852113	15.677082
24.087990	1184.105687	15.682099
23.829851	1177.313941	15.687117
23.913574	1173.869268	15.692135
23.686559	1183.390519	15.697152
23.915089	1176.307361	15.702170
24.209026	1175.853230	15.707187
24.058962	1175.949754	15.712205
24.337559	1177.847569	15.717223
24.210277	1195.412812	15.722240
24.507615	1197.621062	15.727258
24.316008	1198.304671	15.732275
24.078271	1205.254512	15.737293
24.716680	1194.784278	15.742311
24.446330	1200.753057	15.747328
24.401100	1201.322333	15.752346
24.518123	1203.078376	15.757363
24.320764	1201.633563	15.762381
24.660119	1207.159518	15.767399
24.593380	1199.971232	15.772416
24.671907	1202.804522	15.777434
25.059488	1198.412927	15.782451
24.748688	1183.857352	15.787469
24.711559	1184.433162	15.792487
24.621422	1169.319766	15.797504
24.528614	1160.964939	15.802522
24.552777	1164.994407	15.807539
24.468248	1196.721867	15.812557
24.913540	1182.393059	15.817575
24.794336	1193.938090	15.822592
24.922665	1196.425015	15.827610
24.687759	1197.967016	15.832627
24.697092	1195.442945	15.837645
24.728505	1193.432265	15.842663
24.759344	1200.903179	15.847680
24.630704	1196.284542	15.852698
24.691124	1198.804537	15.857715
24.658105	1189.962728	15.862733
24.971512	1177.392832	15.867751
25.038491	1191.344481	15.872768
25.244174	1199.423796	15.877786
25.483150	1190.230790	15.882803
25.053500	1201.858225	15.887821
25.002693	1195.408524	15.892839
24.841523	1193.512727	15.897856
25.139069	1192.537023	15.902874
25.192687	1190.690757	15.907891
24.900300	1195.441921	15.912909
25.082943	1199.039568	15.917927
25.029750	1200.191954	15.922944
24.850556	1204.235356	15.927962
25.489456	1220.615134	15.932979
25.518758	1219.091924	15.937997
25.692783	1216.452263	15.943015
25.620225	1206.279403	15.948032
25.254712	1204.133759	15.953050
25.307575	1198.487852	15.958067
25.045463	1217.648172	15.963085
25.519472	1224.238120	15.968103
25.904000	1227.187158	15.973120
25.715725	1221.226031	15.978138
25.823949	1216.700705	15.983155
25.322967	1212.014876	15.988173
25.705081	1215.589404	15.993191
25.492386	1220.316188	15.998208
25.728958	1216.519528	16.003226
25.806065	1225.811050	16.008243
25.502695	1232.529072	16.013261
25.845259	1214.537892	16.018279
25.864544	1218.942332	16.023296
26.013030	1212.418948	16.028314
26.085108	1222.313562	16.033331
25.720957	1203.272052	16.038349
25.880534	1201.791084	16.043367
25.870012	1191.555039	16.048384
26.009934	1206.141390	16.053402
26.190961	1215.379912	16.058419
26.062096	1192.920561	16.063437
25.845652	1175.578995	16.068455
26.042854	1194.118199	16.073472
25.897088	1204.602449	16.078490
26.354145	1204.986573	16.083507
26.334306	1189.888306	16.088525
25.982604	1180.530954	16.093543
26.051525	1186.756207	16.098560
26.133717	1205.724205	16.103578
26.126556	1217.984474	16.108595
26.144363	1215.697740	16.113613
26.382148	1201.933040	16.118631
26.389800	1216.309013	16.123648
26.393950	1208.720293	16.128666
26.250390	1205.017945	16.133683
26.092788	1211.588072	16.138701
26.342236	1209.016052	16.143719
26.137846	1208.174270	16.148736
26.141598	1214.903923	16.153754
26.259820	1208.945489	16.158771
26.168453	1211.801149	16.163789
26.123600	1209.406089	16.168807
26.182874	1210.792013	16.173824
26.163739	1215.201226	16.178842
26.401366	1214.910312	16.183859
26.779297	1236.309776	16.188877
26.833222	1237.348415	16.193895
27.127323	1232.826023	16.198912
26.618854	1217.471328	16.203930
26.900623	1210.900726	16.208947
26.579390	1212.308003	16.213965
26.875904	1204.926243	16.218983
26.865145	1201.587319	16.224000
26.423220	1202.465615	16.229018
26.722355	1205.624594	16.234035
26.478635	1208.396786	16.239053
26.654887	1218.971114	16.244071
26.948178	1232.580137	16.249088
27.026202	1236.017551	16.254106
26.980249	1223.169264	16.259123
26.674096	1242.074337	16.264141
26.726026	1235.929243	16.269159
26.721012	1226.436630	16.274176
26.665296	1237.312057	16.279194
27.110660	1229.102276	16.284211
26.955867	1230.936502	16.289229
27.038312	1225.761603	16.294247
26.957513	1236.366023	16.299264
26.970635	1245.006624	16.304282
27.242583	1243.908593	16.309299
27.194561	1272.469667	16.314317
27.172752	1273.114788	16.319335
27.342592	1256.564670	16.324352
27.264222	1270.825010	16.329370
27.542406	1266.977767	16.334387
27.664352	1261.757752	16.339405
27.577283	1247.574133	16.344423
27.593234	1261.815138	16.349440
27.295813	1267.170799	16.354458
27.888885	1260.184815	16.359475
27.889956	1256.622897	16.364493
27.165902	1242.258767	16.369511
27.717962	1239.361386	16.374528
27.186278	1244.985242	16.379546
27.876597	1233.705550	16.384563
27.785162	1254.046175	16.389581
27.920175	1257.572192	16.394599
28.033067	1241.670570	16.399616
27.797561	1236.619852	16.404634
27.617024	1227.384554	16.409651
27.540182	1230.079771	16.414669
27.245289	1246.755402	16.419687
27.793825	1246.965184	16.424704
27.708530	1262.628007	16.429722
27.988213	1261.453315	16.434739
27.669931	1262.214544	16.439757
27.534553	1261.423942	16.444775
28.118119	1257.518364	16.449792
27.890942	1264.407638	16.454810
28.068649	1256.352685	16.459827
28.335360	1258.407960	16.464845
28.177657	1256.357277	16.469863
28.271418	1256.682756	16.474880
28.343879	1257.386105	16.479898
28.567675	1265.618341	16.484915
28.675867	1266.087476	16.489933
28.294569	1269.668114	16.494951
28.409616	1260.387886	16.499968
28.219286	1262.321675	16.504986
28.456758	1255.093718	16.510003
28.276417	1262.146287	16.515021
27.927160	1257.687889	16.520039
28.414466	1256.105128	16.525056
28.225248	1259.222793	16.530074
28.311775	1251.692080	16.535091
28.063215	1261.316726	16.540109
28.023223	1258.095005	16.545127
28.183027	1253.402704	16.550144
27.844769	1266.089911	16.555162
28.642705	1270.850455	16.560179
28.616824	1280.217878	16.565197
28.350708	1283.589161	16.570215
28.724973	1287.743060	16.575232
28.523567	1287.959273	16.580250
29.060343	1282.550638	16.585267
28.942099	1283.386864	16.590285
29.027068	1284.117079	16.595303
28.756913	1275.107355	16.600320
28.832375	1282.587270	16.605338
28.849432	1280.958222	16.610355
29.094688	1281.554289	16.615373
29.037881	1284.991164	16.620391
29.026132	1278.687705	16.625408
28.905152	1274.737553	16.630426
29.135370	1275.154638	16.635443
29.271609	1282.407418	16.640461
29.120448	1280.968544	16.645479
29.434616	1274.274470	16.650496
28.543809	1256.435494	16.655514
28.986583	1252.636241	16.660531
28.993367	1274.226991	16.665549
28.677171	1273.738273	16.670567
28.825197	1267.756194	16.675584
28.878596	1281.553108	16.680602
28.935953	1275.958390	16.685619
28.692084	1284.213991	16.690637
28.865095	1301.456547	16.695655
29.408365	1307.261783	16.700672
29.068917	1310.903024	16.705690
28.911650	1301.970677	16.710707
29.758759	1309.582298	16.715725
29.374606	1312.063002	16.720743
29.434142	1299.656791	16.725760
29.510883	1302.807273	16.730778
29.330705	1314.394748	16.735795
29.429129	1311.642583	16.740813
29.624571	1326.316708	16.745831
29.674127	1328.713933	16.750848
30.070532	1324.046085	16.755866
30.214767	1307.703065	16.760883
30.264316	1297.990401	16.765901
30.160879	1295.527659	16.770919
30.285453	1291.111795	16.775936
30.196371	1286.675541	16.780954
30.157772	1291.230292	16.785971
30.351326	1283.567328	16.790989
29.836708	1272.890010	16.796007
30.007984	1260.867268	16.801024
29.776722	1272.825103	16.806042
29.459311	1279.916470	16.811059
29.845701	1287.870118	16.816077
29.895578	1289.302872	16.821095
30.067917	1289.384892	16.826112
30.038396	1288.317388	16.831130
29.955947	1299.665903	16.836147
30.158626	1289.501630	16.841165
30.005052	1298.575255	16.846183
30.029104	1291.132984	16.851200
30.131103	1291.896600	16.856218
30.161272	1288.582582	16.861235
30.145716	1297.295264	16.866253
30.035656	1312.204084	16.871271
30.485544	1315.333056	16.876288
30.600344	1329.075975	16.881306
30.769249	1329.896636	16.886323
30.555009	1322.282541	16.891341
30.379255	1325.410984	16.896359
30.660476	1315.851923	16.901376
30.534668	1310.605521	16.906394
30.236146	1324.160086	16.911411
30.656273	1316.244738	16.916429
30.261360	1324.341295	16.921447
30.577077	1314.346288	16.926464
30.456000	1312.615870	16.931482
30.343527	1316.987986	16.936499
30.659593	1320.339042	16.941517
30.768621	1321.936602	16.946535
30.919495	1321.847985	16.951552
30.930536	1316.417574	16.956570
30.335259	1337.204899	16.961587
30.652572	1326.067673	16.966605
30.664534	1349.861855	16.971623
31.120600	1359.102840	16.976640
31.377260	1354.864312	16.981658
31.422775	1355.091287	16.986675
31.092392	1334.945384	16.991693
30.738575	1335.953395	16.996711
31.142258	1342.748687	17.001728
31.236348	1340.983693	17.006746
31.071499	1352.307878	17.011763
31.242381	1343.594267	17.016781
31.229246	1353.583153	17.021799
31.174533	1351.772680	17.026816
31.673258	1346.616927	17.031834
31.516580	1348.270799	17.036851
31.797050	1336.504911	17.041869
31.389672	1354.552775	17.046887
31.720648	1343.291054	17.051904
31.655903	1317.925904	17.056922
31.238186	1309.377287	17.061939
31.576388	1323.050217	17.066957
31.533839	1342.040572	17.071975
31.256088	1340.547427	17.076992
31.474212	1340.474857	17.082010
31.314007	1346.196391	17.087027
31.330525	1349.053536	17.092045
31.530222	1338.944438	17.097063
31.615281	1343.526991	17.102080
31.340543	1340.498942	17.107098
31.426406	1350.082747	17.112115
31.736541	1355.566152	17.117133
31.637682	1367.376609	17.122151
31.508848	1369.105199	17.127168
31.946739	1371.280211	17.132186
31.908544	1361.666443	17.137203
32.299560	1360.388713	17.142221
31.862304	1364.855059	17.147239
32.020308	1359.388538	17.152256
32.122806	1368.647412	17.157274
32.042304	1366.200156	17.162291
32.110749	1350.185314	17.167309
31.648524	1358.195390	17.172327
32.018124	1356.511421	17.177344
32.159908	1352.814828	17.182362
32.380661	1388.790189	17.187379
32.969655	1377.163807	17.192397
32.730057	1365.066779	17.197415
32.593596	1365.272849	17.202432
32.528329	1341.495887	17.207450
32.371854	1354.483193	17.212467
32.591831	1342.992806	17.217485
32.582534	1341.265957	17.222503
32.564167	1344.509712	17.227520
32.546655	1341.354522	17.232538
32.280129	1342.148337	17.237555
32.644797	1344.111267	17.242573
32.531583	1341.309045	17.247591
32.437855	1344.547736	17.252608
32.943729	1337.976065	17.257626
32.533704	1345.676571	17.262643
32.873383	1346.430042	17.267661
32.895390	1337.301145	17.272679
32.758858	1341.760892	17.277696
33.016588	1334.629929	17.282714
32.421016	1351.706882	17.287731
33.052029	1356.953431	17.292749
32.937923	1373.046850	17.297767
33.065932	1375.709028	17.302784
32.934040	1361.655526	17.307802
32.926598	1367.644298	17.312819
32.880646	1373.451080	17.317837
32.877764	1373.964356	17.322855
33.197123	1363.404433	17.327872
33.372903	1370.556444	17.332890
33.207381	1361.686637	17.337907
33.445934	1366.068464	17.342925
33.128643	1373.923516	17.347943
33.289160	1376.931449	17.352960
33.452552	1380.048339	17.357978
33.304009	1378.943026	17.362995
33.332679	1366.258047	17.368013
33.236212	1377.154675	17.373031
33.050147	1374.212147	17.378048
33.582574	1362.496911	17.383066
33.622193	1395.740249	17.388083
33.339616	1395.015888	17.393101
33.490466	1396.562063	17.398119
33.277434	1398.594094	17.403136
33.455838	1388.534933	17.408154
33.449791	1402.935782	17.413171
33.860247	1408.728759	17.418189
33.657752	1396.230556	17.423207
33.239656	1394.627940	17.428224
33.874735	1398.185508	17.433242
33.882296	1417.643193	17.438259
34.085746	1425.933595	17.443277
34.131758	1412.969376	17.448295
34.008882	1400.086415	17.453312
34.026384	1399.219959	17.458330
34.084772	1404.343273	17.463347
34.441601	1404.315291	17.468365
34.305494	1395.529960	17.473383
34.199702	1391.528654	17.478400
34.234359	1384.127098	17.483418
34.165727	1379.163305	17.488435
34.449894	1380.462089	17.493453
34.564544	1386.939866	17.498471
34.378860	1384.214759	17.503488
34.242390	1383.794354	17.508506
34.297674	1387.403644	17.513523
34.129400	1374.248525	17.518541
34.450809	1391.684146	17.523559
34.720592	1417.328057	17.528576
34.769870	1417.438090	17.533594
34.743578	1408.924914	17.538611
34.715712	1388.126285	17.543629
34.735803	1390.673445	17.548647
34.582514	1386.549694	17.553664
34.888480	1381.454126	17.558682
34.571062	1390.933170	17.563699
34.582898	1382.544200	17.568717
34.487955	1395.755588	17.573735
34.879363	1413.189900	17.578752
35.204242	1407.985898	17.583770
34.820494	1410.631289	17.588787
34.895652	1418.735832	17.593805
34.994290	1419.811577	17.598823
34.726469	1423.359326	17.603840
34.859862	1413.401273	17.608858
34.997031	1427.863309	17.613875
35.061180	1421.230368	17.618893
34.890598	1416.675084	17.623911
35.008948	1405.586229	17.628928
35.017459	1412.920012	17.633946
35.015232	1408.933471	17.638963
35.199852	1416.411552	17.643981
35.031192	1407.986658	17.648999
34.803752	1424.509623	17.654016
34.891193	1438.882068	17.659034
34.928208	1439.709374	17.664051
34.892120	1443.329644	17.669069
34.955820	1439.927584	17.674087
35.296732	1459.552446	17.679104
36.052124	1465.352607	17.684122
35.705317	1468.640822	17.689139
35.967869	1451.658700	17.694157
36.129997	1443.297215	17.699175
35.981867	1432.153574	17.704192
35.906294	1426.382176	17.709210
35.859772	1424.917729	17.714227
35.837517	1429.745370	17.719245
36.063174	1416.034443	17.724263
35.793313	1434.472408	17.729280
36.055766	1425.455474	17.734298
36.053217	1415.416160	17.739315
36.232453	1428.820420	17.744333
36.264244	1417.627769	17.749351
36.603603	1423.183522	17.754368
36.592874	1425.539355	17.759386
36.228031	1421.066557	17.764403
36.410219	1406.236024	17.769421
36.263515	1416.215139	17.774439
36.200252	1424.805482	17.779456
36.306266	1417.258674	17.784474
36.428045	1418.678376	17.789491
36.242908	1429.316508	17.794509
36.116088	1419.057016	17.799527
35.984288	1426.390767	17.804544
36.185165	1417.053354	17.809562
36.327957	1426.187118	17.814579
36.276514	1425.640079	17.819597
36.465949	1423.591447	17.824615
36.399277	1425.543987	17.829632
36.363242	1406.914466	17.834650
36.675713	1437.101451	17.839667
36.665101	1445.978730	17.844685
36.718006	1444.898972	17.849703
36.769900	1456.514729	17.854720
37.037694	1448.657946	17.859738
36.785182	1453.565567	17.864755
36.665725	1454.637401	17.869773
36.871128	1448.330266	17.874791
36.766773	1455.545733	17.879808
36.930599	1448.281439	17.884826
36.784753	1444.839608	17.889843
36.790556	1457.075095	17.894861
36.901307	1458.140771	17.899879
37.007220	1455.052353	17.904896
37.179925	1449.326717	17.909914
36.822720	1446.517755	17.914931
36.903062	1446.289634	17.919949
37.226165	1454.946835	17.924967
37.485676	1471.283688	17.929984
37.471918	1481.736471	17.935002
37.569396	1469.421083	17.940019
37.313355	1477.122779	17.945037
37.526074	1472.332705	17.950055
37.542535	1467.780939	17.955072
37.534203	1481.337484	17.960090
37.762784	1478.987930	17.965107
37.903866	1465.039005	17.970125
37.647965	1436.006389	17.975143
37.400035	1448.961454	17.980160
37.655516	1454.976092	17.985178
37.983124	1458.564016	17.990195
37.979948	1459.843175	17.995213
38.075695	1470.564426	18.000231
37.676586	1458.198845	18.005248
37.986045	1470.465647	18.010266
37.996568	1473.635176	18.015283
37.749142	1473.387412	18.020301
38.192192	1462.506237	18.025319
37.996790	1476.573147	18.030336
37.568606	1474.449629	18.035354
37.763051	1474.860035	18.040371
37.807854	1467.236323	18.045389
37.945889	1464.124292	18.050407
37.716274	1473.252706	18.055424
37.964699	1477.997644	18.060442
38.170460	1491.245827	18.065459
38.169290	1500.329814	18.070477
38.433407	1502.831747	18.075495
38.635971	1499.872406	18.080512
38.740856	1496.909723	18.085530
38.720644	1495.292912	18.090547
38.654775	1494.911419	18.095565
38.816466	1493.277341	18.100583
38.875893	1492.044556	18.105600
38.742883	1486.695362	18.110618
39.015880	1486.589121	18.115635
38.781471	1480.809114	18.120653
38.899115	1452.932667	18.125671
38.681927	1457.742931	18.130688
38.675808	1467.946054	18.135706
38.951793	1475.592503	18.140723
38.470884	1482.220699	18.145741
39.007712	1480.607296	18.150759
39.011976	1493.420934	18.155776
38.895012	1498.845067	18.160794
39.007770	1491.290811	18.165811
39.017343	1486.488837	18.170829
39.112240	1474.895221	18.175847
39.236950	1486.232275	18.180864
39.105216	1476.876179	18.185882
38.966159	1480.528235	18.190899
38.876620	1484.751551	18.195917
39.007432	1485.885164	18.200935
39.193102	1500.709869	18.205952
39.463744	1502.896202	18.210970
39.754631	1515.078720	18.215987
39.378231	1501.631358	18.221005
39.303167	1506.410081	18.226023
39.637118	1507.091289	18.231040
39.701043	1516.270025	18.236058
39.715614	1501.025038	18.241075
39.784351	1515.830898	18.246093
39.480901	1520.560174	18.251111
39.647119	1509.037805	18.256128
39.753744	1502.481065	18.261146
40.091874	1514.056847	18.266163
39.562999	1522.542324	18.271181
39.907646	1511.323885	18.276199
39.608741	1504.700910	18.281216
39.372856	1504.666560	18.286234
39.944722	1511.053679	18.291251
39.776000	1531.103943	18.296269
40.139766	1528.557659	18.301287
40.631857	1535.248087	18.306304
40.550684	1529.505131	18.311322
40.522307	1507.084808	18.316339
40.377563	1510.740763	18.321357
40.345839	1500.408423	18.326375
40.317354	1504.308512	18.331392
40.091536	1500.343545	18.336410
40.730799	1505.574809	18.341427
40.381989	1519.060899	18.346445
40.429747	1517.647586	18.351463
40.607880	1529.539738	18.356480
40.232822	1540.213660	18.361498
40.670125	1529.277294	18.366515
40.545620	1534.803853	18.371533
40.692568	1531.426987	18.376551
40.634414	1522.704871	18.381568
40.442398	1522.546359	18.386586
40.902660	1521.960616	18.391603
40.875419	1536.894742	18.396621
40.769203	1527.468660	18.401639
40.954440	1533.861223	18.406656
40.650090	1532.932806	18.411674
41.008661	1518.324753	18.416691
40.940886	1529.441518	18.421709
40.837841	1538.815749	18.426727
41.152250	1556.830387	18.431744
41.177035	1554.339722	18.436762
41.463020	1561.035288	18.441779
41.442609	1547.916994	18.446797
41.421990	1553.454734	18.451815
41.355890	1550.391771	18.456832
41.168640	1548.114664	18.461850
41.250125	1546.636925	18.466867
41.259434	1550.210354	18.471885
41.591986	1549.029463	18.476903
41.461938	1545.568268	18.481920
41.347686	1558.684379	18.486938
41.284537	1545.727262	18.491955
41.529989	1548.764297	18.496973
41.475981	1549.389360	18.501991
41.693673	1549.034028	18.507008
41.833271	1570.033250	18.512026
41.708538	1567.450575	18.517043
41.616733	1576.539546	18.522061
41.846392	1562.039554	18.527079
42.076171	1560.595765	18.532096
42.349698	1569.582437	18.537114
42.514346	1565.705072	18.542131
42.348337	1573.029194	18.547149
42.083407	1569.467859	18.552167
42.551287	1562.610288	18.557184
42.453957	1554.710457	18.562202
42.578861	1553.636704	18.567219
42.427192	1543.220038	18.572237
42.627967	1529.581813	18.577255
42.389863	1526.682495	18.582272
42.614354	1532.772551	18.587290
42.932760	1524.799507	18.592307
42.761137	1530.741272	18.597325
42.571086	1531.747819	18.602343
42.578198	1520.947500	18.607360
42.424111	1534.450630	18.612378
42.546857	1532.019950	18.617395
42.468124	1518.272828	18.622413
42.249754	1530.609386	18.627431
42.702017	1537.843721	18.632448
42.610225	1558.396392	18.637466
42.767440	1564.028550	18.642483
42.913430	1564.657566	18.647501
42.823102	1559.546731	18.652519
42.979054	1561.508950	18.657536
42.887167	1567.691848	18.662554
43.161835	1561.554691	18.667571
42.763921	1565.701054	18.672589
42.958128	1563.929331	18.677607
43.112819	1561.263086	18.682624
42.802585	1566.373758	18.687642
43.216697	1581.655406	18.692659
43.245374	1590.811669	18.697677
42.994509	1592.413817	18.702695
43.570307	1600.677423	18.707712
43.143468	1600.641956	18.712730
43.139765	1591.074502	18.717747
43.075533	1592.517677	18.722765
43.205271	1602.300463	18.727783
43.229081	1615.960658	18.732800
43.237737	1619.249014	18.737818
43.571579	1618.671562	18.742835
43.660004	1621.672365	18.747853
44.113822	1615.552032	18.752871
44.066247	1612.648374	18.757888
44.165762	1617.986586	18.762906
44.361362	1614.583751	18.767923
43.915925	1613.378094	18.772941
43.940666	1611.273003	18.777959
44.458207	1613.071948	18.782976
44.207345	1618.493450	18.787994
44.592595	1614.988616	18.793011
44.313724	1608.302451	18.798029
44.460804	1616.054316	18.803047
44.301614	1612.884102	18.808064
44.202340	1614.149828	18.813082
44.438538	1612.235747	18.818099
44.265312	1618.051056	18.823117
44.198527	1607.729752	18.828135
44.482343	1607.511700	18.833152
44.179955	1620.030693	18.838170
44.277187	1603.148548	18.843187
44.430464	1620.489789	18.848205
44.605654	1637.008841	18.853223
45.180652	1635.008852	18.858240
45.354387	1641.133517	18.863258
44.784543	1629.690180	18.868275
45.074350	1622.151280	18.873293
44.694202	1624.571929	18.878311
45.057383	1632.497118	18.883328
44.783480	1646.352777	18.888346
45.060081	1641.597561	18.893363
45.168383	1636.492059	18.898381
45.259830	1633.001919	18.903399
45.312810	1625.273642	18.908416
45.005733	1635.164258	18.913434
45.126620	1637.147437	18.918451
45.139984	1630.590702	18.923469
44.892693	1640.968027	18.928487
45.397760	1647.475480	18.933504
45.311907	1628.086310	18.938522
45.412659	1637.291706	18.943539
45.352796	1635.303728	18.948557
45.468296	1628.702363	18.953575
45.271381	1637.394428	18.958592
45.315881	1664.843259	18.963610
45.864316	1666.092690	18.968627
46.162718	1667.544047	18.973645
46.053846	1667.718597	18.978663
46.606852	1662.045376	18.983680
45.921578	1643.826356	18.988698
46.091328	1630.790134	18.993715
46.192855	1633.399457	18.998733
45.949998	1620.946514	19.003751
46.074721	1629.879674	19.008768
45.648964	1631.065119	19.013786
45.740582	1635.290228	19.018803
45.871239	1650.064335	19.023821
45.999198	1667.969973	19.028839
46.215226	1654.512951	19.033856
46.135547	1666.120101	19.038874
46.390875	1663.933991	19.043891
46.398841	1649.287703	19.048909
46.256541	1667.095304	19.053927
46.481715	1658.283580	19.058944
46.105881	1668.677639	19.063962
46.480390	1678.582798	19.068979
46.481776	1677.255864	19.073997
46.709258	1675.472528	19.079015
46.564550	1684.169769	19.084032
46.631890	1689.454276	19.089050
46.908524	1675.562473	19.094067
47.043079	1684.750699	19.099085
46.662686	1678.126549	19.104103
47.073246	1666.426302	19.109120
47.088811	1671.527259	19.114138
47.143975	1673.728362	19.119155
47.267597	1668.540211	19.124173
47.131124	1676.243308	19.129191
47.257361	1675.546835	19.134208
47.248954	1672.628229	19.139226
47.179903	1688.707054	19.144243
47.537916	1697.133063	19.149261
47.507611	1702.991116	19.154279
48.019145	1701.785952	19.159296
47.786158	1685.061619	19.164314
47.702277	1675.121784	19.169331
48.015786	1667.405741	19.174349
48.023578	1668.812812	19.179367
47.832132	1660.599782	19.184384
47.763197	1659.595254	19.189402
47.329277	1669.793626	19.194419
47.667862	1654.864972	19.199437
47.630768	1667.022687	19.204455
47.869989	1688.127442	19.209472
47.920773	1698.719097	19.214490
47.911536	1691.477382	19.219507
48.196897	1693.552271	19.224525
47.987328	1704.187347	19.229543
48.088929	1684.995445	19.234560
47.825557	1695.007993	19.239578
47.830966	1698.112478	19.244595
48.153592	1689.819600	19.249613
48.050957	1699.842397	19.254631
48.526822	1702.761083	19.259648
48.329777	1723.448084	19.264666
48.247846	1723.792176	19.269683
48.265153	1711.898252	19.274701
47.932645	1722.990803	19.279719
48.204979	1721.837762	19.284736
48.383525	1714.138291	19.289754
48.225892	1718.331984	19.294771
48.867074	1739.841780	19.299789
48.667539	1749.467289	19.304807
49.151178	1746.670089	19.309824
49.347583	1751.308763	19.314842
49.255546	1742.401202	19.319859
49.468317	1720.647712	19.324877
49.184149	1710.809447	19.329895
48.756897	1715.046513	19.334912
49.359607	1712.390644	19.339930
49.225486	1732.476786	19.344947
49.137262	1728.159734	19.349965
49.015937	1739.065843	19.354983
49.336049	1743.677184	19.360000
49.194383	1746.007662	19.365018
49.131744	1738.812344	19.370035
49.655155	1742.905113	19.375053
49.308671	1747.737029	19.380071
49.632785	1731.612620	19.385088
49.494727	1739.799608	19.390106
49.466685	1749.724294	19.395123
49.578799	1744.908838	19.400141
49.491380	1749.102352	19.405159
49.869871	1760.003037	19.410176
49.774811	1762.055575	19.415194
49.699764	1755.478165	19.420211
50.340400	1753.100828	19.425229
49.916618	1771.374695	19.430247
50.045104	1761.690815	19.435264
50.109206	1746.204359	19.440282
49.905388	1756.256312	19.445299
49.987908	1757.044428	19.450317
50.055154	1756.412221	19.455335
50.335061	1771.860706	19.460352
50.345555	1776.351983	19.465370
50.820502	1793.910112	19.470387
50.766801	1789.121058	19.475405
50.854511	1782.046132	19.480423
50.739414	1768.361087	19.485440
50.954632	1759.012044	19.490458
50.533690	1763.889139	19.495475
50.772452	1745.184864	19.500493
50.763873	1761.507675	19.505511
51.142275	1772.547145	19.510528
51.096531	1756.181506	19.515546
50.487490	1744.764832	19.520563
51.040410	1764.603838	19.525581
50.871365	1774.282388	19.530599
51.256386	1776.571105	19.535616
51.170454	1785.367140	19.540634
50.987670	1783.484485	19.545651
51.361265	1767.675835	19.550669
51.151530	1781.107679	19.555687
51.213265	1770.643389	19.560704
51.263288	1768.993489	19.565722
51.297758	1772.724996	19.570739
51.347483	1769.292303	19.575757
51.438469	1773.204406	19.580775
51.827150	1778.083328	19.585792
51.701558	1779.980304	19.590810
51.611339	1794.953234	19.595827
52.105261	1788.870689	19.600845
51.771653	1782.161016	19.605863
51.823940	1777.079487	19.610880
52.034925	1788.340901	19.615898
51.702479	1788.482722	19.620915
52.196808	1790.238286	19.625933
52.189751	1802.499792	19.630951
52.036604	1802.284663	19.635968
52.349552	1796.068263	19.640986
51.983545	1802.079651	19.646003
52.129715	1790.008093	19.651021
52.300643	1804.065153	19.656039
52.319924	1797.155839	19.661056
52.565874	1795.794778	19.666074
52.293837	1796.915664	19.671091
52.267847	1790.334069	19.676109
52.313717	1799.920040	19.681127
52.248738	1802.010914	19.686144
52.428936	1798.990851	19.691162
52.120350	1824.547184	19.696179
52.551608	1826.325378	19.701197
52.634150	1820.702091	19.706215
52.527125	1834.660838	19.711232
53.172161	1828.984157	19.716250
52.997502	1830.098795	19.721267
53.217940	1838.204746	19.726285
53.134166	1818.689221	19.731303
52.989232	1820.224090	19.736320
53.173000	1830.139808	19.741338
52.896401	1838.330256	19.746355
53.101871	1840.724235	19.751373
53.330948	1853.285892	19.756391
53.575873	1852.842993	19.761408
53.827091	1847.968892	19.766426
53.747118	1858.739528	19.771443
53.862942	1843.203291	19.776461
53.868612	1848.942280	19.781479
53.642564	1858.057538	19.786496
53.747492	1853.766596	19.791514
53.836566	1851.805153	19.796531
53.959796	1843.709493	19.801549
53.808292	1843.235069	19.806567
53.812804	1835.415889	19.811584
54.035684	1833.284915	19.816602
53.629176	1848.499116	19.821619
53.545667	1834.324010	19.826637
53.868517	1841.020890	19.831655
53.676322	1864.876571	19.836672
54.583660	1861.648355	19.841690
54.141293	1869.945731	19.846707
54.533386	1856.106332	19.851725
54.645931	1859.734024	19.856743
54.392117	1864.024152	19.861760
54.711782	1854.654445	19.866778
54.476109	1876.595716	19.871795
54.836889	1870.805383	19.876813
54.949108	1864.082034	19.881831
54.532344	1870.429749	19.886848
54.733987	1867.139823	19.891866
54.884790	1856.346819	19.896883
55.126439	1857.839066	19.901901
55.171583	1851.460033	19.906919
54.606653	1865.378152	19.911936
54.982636	1860.956206	19.916954
54.961928	1856.100860	19.921971
54.774652	1870.427778	19.926989
55.449630	1880.964240	19.932007
55.034175	1882.933731	19.937024
55.249871	1886.107823	19.942042
55.089395	1899.225170	19.947059
55.407881	1884.147075	19.952077
55.599863	1884.811413	19.957095
55.246451	1883.852305	19.962112
55.625449	1880.447646	19.967130
55.673363	1891.245394	19.972147
55.522632	1889.278108	19.977165
55.641261	1883.848219	19.982183
55.507531	1896.318112	19.987200
56.127297	1901.670440	19.992218
55.928742	1904.533901	19.997235
55.876135	1918.820305	20.002253
55.876944	1924.906935	20.007271
55.740884	1921.126608	20.012288
55.993407	1916.194206	20.017306
56.069645	1918.052335	20.022323
56.170572	1912.169708	20.027341
56.331469	1900.597539	20.032359
56.294647	1909.628217	20.037376
56.382830	1905.987785	20.042394
56.308811	1913.000839	20.047411
56.620330	1928.897748	20.052429
56.916921	1930.091587	20.057447
56.938252	1944.481728	20.062464
57.148254	1926.936574	20.067482
56.806992	1908.200602	20.072499
56.849852	1915.332909	20.077517
56.803008	1910.838319	20.082535
57.006809	1926.135382	20.087552
57.133375	1935.957090	20.092570
57.033376	1937.192256	20.097587
56.937275	1935.233257	20.102605
57.323591	1933.187847	20.107623
57.003767	1941.783871	20.112640
57.453698	1932.196551	20.117658
57.314914	1935.892561	20.122675
57.084892	1935.867672	20.127693
57.540905	1930.624309	20.132711
57.383162	1932.579760	20.137728
57.192972	1927.233562	20.142746
57.403913	1940.007120	20.147763
57.109776	1955.620918	20.152781
58.087232	1958.632535	20.157799
57.636007	1966.300200	20.162816
58.220309	1956.969565	20.167834
58.058522	1950.218238	20.172851
58.139669	1954.049739	20.177869
58.316612	1957.407000	20.182887
58.048813	1956.081222	20.187904
58.235996	1946.633954	20.192922
58.514870	1956.331896	20.197939
58.274119	1955.813955	20.202957
58.593724	1948.779166	20.207975
58.230530	1947.319760	20.212992
58.734414	1951.214460	20.218010
58.519830	1940.397338	20.223027
58.488826	1944.601069	20.228045
58.628120	1953.482999	20.233063
58.395412	1944.127361	20.238080
58.478166	1946.640836	20.243098
58.693622	1938.539727	20.248115
58.525164	1940.618983	20.253133
58.922091	1956.955691	20.258151
58.491602	1968.292732	20.263168
58.739450	1966.302282	20.268186
59.076391	1966.976524	20.273203
58.752376	1989.094542	20.278221
58.922222	1972.103154	20.283239
59.060176	1976.794465	20.288256
58.737587	1984.471194	20.293274
59.385012	1991.798678	20.298291
59.280011	2007.309628	20.303309
59.557809	2012.579741	20.308327
59.494131	2003.283527	20.313344
59.636022	2005.042245	20.318362
59.544489	2006.686404	20.323379
60.007702	1998.359502	20.328397
59.969821	2005.962424	20.333415
59.599619	2000.760501	20.338432
59.767172	1998.408752	20.343450
59.891736	2003.770712	20.348467
59.621063	1987.176475	20.353485
60.056562	1994.520676	20.358503
59.908980	2010.426023	20.363520
59.864048	2006.383400	20.368538
60.054755	2010.900472	20.373555
60.146606	2023.238712	20.378573
60.225010	2010.652058	20.383591
60.391851	2017.355703	20.388608
60.508186	2016.523663	20.393626
60.647143	2015.071812	20.398643
60.339407	2021.932220	20.403661
60.625545	2010.420562	20.408679
60.456456	2023.022567	20.413696
60.498065	2028.383482	20.418714
60.895210	2037.855852	20.423731
60.595289	2054.088943	20.428749
61.128802	2049.311028	20.433767
61.073470	2050.337860	20.438784
60.942299	2040.578812	20.443802
61.059651	2037.728126	20.448819
60.989642	2036.588136	20.453837
61.082279	2030.829457	20.458855
61.492839	2043.266606	20.463872
61.477175	2049.429030	20.468890
61.562458	2048.749937	20.473907
61.724952	2053.588775	20.478925
62.018896	2046.842599	20.483943
61.609912	2037.867176	20.488960
61.683538	2044.961785	20.493978
61.949901	2052.569567	20.498995
61.548906	2056.851003	20.504013
62.229432	2056.790594	20.509031
61.893173	2059.329042	20.514048
62.202692	2052.273631	20.519066
62.056807	2052.844219	20.524083
62.052511	2061.721991	20.529101
62.238303	2051.836354	20.534119
62.408704	2048.365156	20.539136
62.348907	2061.579574	20.544154
62.480157	2057.929037	20.549171
62.427509	2056.164985	20.554189
62.682586	2055.831414	20.559207
62.601918	2055.208088	20.564224
62.503467	2058.879157	20.569242
62.655852	2055.268234	20.574259
62.371340	2052.296965	20.579277
62.549911	2056.703666	20.584295
62.699398	2071.202065	20.589312
62.813311	2081.379264	20.594330
62.858389	2079.569142	20.599347
63.082217	2091.173107	20.604365
63.392483	2081.393247	20.609383
63.512608	2078.172450	20.614400
63.234111	2086.821167	20.619418
63.518672	2086.160909	20.624435
63.335177	2085.494737	20.629453
63.624453	2077.370532	20.634471
63.761258	2084.607459	20.639488
63.384451	2081.903180	20.644506
63.644915	2070.060324	20.649523
63.469499	2078.845530	20.654541
63.504724	2075.216171	20.659559
63.637981	2073.312943	20.664576
63.378471	2082.702928	20.669594
63.760410	2079.176493	20.674611
63.837596	2101.135668	20.679629
63.945348	2105.177552	20.684647
64.033065	2103.046635	20.689664
64.279254	2102.305127	20.694682
64.236141	2097.737235	20.699699
64.100254	2109.158556	20.704717
64.330469	2101.356466	20.709735
64.303962	2087.578160	20.714752
63.979519	2094.539972	20.719770
64.426171	2109.408153	20.724787
64.533153	2119.880390	20.729805
64.309158	2116.931191	20.734823
64.568848	2119.183788	20.739840
64.302567	2125.910634	20.744858
64.524487	2123.021197	20.749875
64.641692	2147.992208	20.754893
64.825046	2139.891575	20.759911
65.147087	2146.251946	20.764928
65.183827	2149.259425	20.769946
65.450600	2152.426116	20.774963
65.125132	2148.335926	20.779981
65.245436	2138.464402	20.784999
65.459421	2144.887900	20.790016
65.530940	2148.797805	20.795034
65.706313	2139.551366	20.800051
65.718874	2145.856590	20.805069
65.854517	2145.125475	20.810087
65.840535	2133.107277	20.815104
65.553463	2143.257679	20.820122
65.830987	2138.112436	20.825139
65.931137	2154.629879	20.830157
66.335362	2163.604358	20.835175
66.524472	2159.546836	20.840192
66.154667	2144.149594	20.845210
66.397697	2139.268292	20.850227
66.292483	2142.653914	20.855245
66.062066	2148.315111	20.860263
66.553311	2150.658175	20.865280
66.377279	2170.103849	20.870298
66.578028	2166.436094	20.875315
66.375703	2168.612895	20.880333
66.423652	2175.056167	20.885351
66.694342	2166.549002	20.890368
66.643185	2170.976377	20.895386
66.997550	2169.201938	20.900403
66.924084	2164.842761	20.905421
66.988209	2168.310435	20.910439
66.833789	2166.653532	20.915456
66.876747	2170.929346	20.920474
67.446034	2180.728243	20.925491
67.230183	2197.496356	20.930509
67.254007	2190.724880	20.935527
67.256717	2189.943099	20.940544
67.098285	2203.297547	20.945562
66.985834	2190.690912	20.950579
67.026888	2188.758226	20.955597
67.530170	2223.275219	20.960615
67.595692	2218.565336	20.965632
67.765053	2219.547963	20.970650
67.770166	2215.764508	20.975667
67.757603	2217.865278	20.980685
68.095356	2207.926088	20.985703
68.547745	2210.769037	20.990720
68.520482	2211.534968	20.995738
69.179254	2197.738392	21.000755
68.737024	2195.721410	21.005773
68.678686	2169.075579	21.010791
68.528640	2165.096538	21.015808
68.284333	2166.913976	21.020826
68.431464	2167.443234	21.025843
68.472876	2170.712123	21.030861
68.594866	2192.902977	21.035879
68.676062	2193.956268	21.040896
68.711666	2205.069035	21.045914
68.869643	2200.331283	21.050931
68.934945	2200.582557	21.055949
68.560791	2203.092649	21.060967
68.647448	2195.074298	21.065984
68.896255	2205.690463	21.071002
68.993763	2205.318171	21.076019
69.200604	2219.222250	21.081037
69.067059	2240.328936	21.086055
69.557718	2228.419970	21.091072
69.143549	2225.677552	21.096090
69.174956	2227.674611	21.101107
69.412785	2229.403724	21.106125
69.565853	2234.496907	21.111143
69.787908	2238.591781	21.116160
69.379107	2255.152100	21.121178
69.636002	2243.944876	21.126195
69.955047	2251.507835	21.131213
69.830269	2257.894456	21.136231
70.194075	2255.704117	21.141248
70.369437	2256.850306	21.146266
70.272782	2249.497393	21.151283
70.031389	2253.914106	21.156301
70.305499	2259.216408	21.161319
70.556060	2274.198247	21.166336
70.456258	2288.522120	21.171354
70.751517	2276.136991	21.176371
70.859319	2280.746772	21.181389
70.825674	2280.335133	21.186407
71.028314	2273.171705	21.191424
71.206408	2285.494330	21.196442
71.156524	2272.039573	21.201459
71.021074	2271.464657	21.206477
70.964360	2284.470312	21.211495
70.964535	2266.313247	21.216512
71.251873	2268.962047	21.221530
71.082053	2281.541354	21.226547
71.367066	2268.569987	21.231565
71.157536	2266.660788	21.236583
71.253129	2280.358722	21.241600
71.436778	2293.674829	21.246618
71.512200	2294.068514	21.251635
71.729148	2304.628207	21.256653
71.894671	2307.444177	21.261671
71.746928	2299.492456	21.266688
71.677889	2303.895071	21.271706
71.741939	2305.725343	21.276723
71.651890	2302.558717	21.281741
71.885179	2313.723729	21.286759
72.209315	2329.532756	21.291776
72.122825	2338.202636	21.296794
72.250083	2330.084404	21.301811
72.215131	2332.927601	21.306829
72.266003	2337.657230	21.311847
72.632040	2319.651437	21.316864
72.352196	2323.300776	21.321882
72.214228	2345.521619	21.326899
72.710569	2347.509574	21.331917
73.180088	2358.234635	21.336935
73.314695	2356.690567	21.341952
73.286509	2354.705135	21.346970
73.324060	2347.554584	21.351987
73.707132	2350.321031	21.357005
72.934622	2345.585826	21.362023
73.341791	2337.363861	21.367040
73.302926	2345.657799	21.372058
73.418872	2352.127110	21.377075
73.676665	2351.851545	21.382093
73.489872	2351.539614	21.387111
73.831094	2351.674240	21.392128
73.641654	2346.438784	21.397146
73.915109	2351.306620	21.402163
73.426928	2349.022235	21.407181
73.191361	2352.261939	21.412199
73.504599	2354.119735	21.417216
74.019530	2380.108371	21.422234
73.676222	2374.947934	21.427251
74.073714	2367.512916	21.432269
74.150616	2372.842727	21.437287
74.336083	2374.636213	21.442304
74.444885	2389.219580	21.447322
74.240623	2408.036218	21.452339
74.763847	2402.003904	21.457357
74.447368	2393.678084	21.462375
74.594933	2390.047802	21.467392
74.770331	2394.018550	21.472410
74.671657	2393.549156	21.477427
74.980909	2395.706604	21.482445
74.966435	2401.818781	21.487463
75.048225	2408.836625	21.492480
75.389077	2414.960556	21.497498
75.415354	2416.118402	21.502515
75.266895	2406.215929	21.507533
75.378460	2408.000177	21.512551
75.719597	2413.055453	21.517568
75.493542	2413.363537	21.522586
75.577156	2410.440215	21.527603
75.352696	2407.693775	21.532621
75.453489	2421.013448	21.537639
75.846098	2423.854113	21.542656
76.159660	2441.658532	21.547674
76.141728	2449.341638	21.552691
76.301847	2433.074124	21.557709
76.284555	2443.774186	21.562727
76.618699	2437.413685	21.567744
76.725512	2444.325844	21.572762
76.755486	2454.878548	21.577779
76.883142	2430.209434	21.582797
76.559467	2431.344407	21.587815
76.310233	2443.162232	21.592832
76.067626	2440.791193	21.597850
76.665443	2436.921946	21.602867
77.050082	2430.466497	21.607885
76.990707	2434.739413	21.612903
76.744232	2432.644582	21.617920
77.074886	2443.218649	21.622938
77.052203	2459.695502	21.627955
77.121994	2458.413491	21.632973
77.060657	2473.635238	21.637991
77.554944	2467.111265	21.643008
77.255003	2468.815303	21.648026
77.170499	2463.465035	21.653043
77.339586	2465.196480	21.658061
77.300514	2479.386489	21.663079
77.546638	2488.504008	21.668096
77.824082	2495.952122	21.673114
78.001270	2487.483655	21.678131
78.004417	2484.125621	21.683149
77.835443	2483.608003	21.688167
78.169321	2489.778389	21.693184
78.171426	2483.054268	21.698202
78.080057	2486.191241	21.703219
78.544565	2494.959907	21.708237
78.510232	2498.140209	21.713255
78.471701	2507.680534	21.718272
78.779672	2510.513747	21.723290
78.681671	2510.776068	21.728307
78.834862	2503.733098	21.733325
78.288960	2513.428324	21.738343
78.695853	2512.662802	21.743360
78.918721	2507.567411	21.748378
78.831977	2514.703500	21.753395
78.965740	2520.186355	21.758413
78.955215	2529.249268	21.763431
79.237999	2538.339894	21.768448
79.473813	2535.804947	21.773466
79.455776	2537.106335	21.778483
79.743327	2534.827976	21.783501
79.719695	2531.684773	21.788519
79.515043	2524.601524	21.793536
79.597725	2541.278161	21.798554
79.731278	2556.491995	21.803571
79.882162	2549.915294	21.808589
80.205609	2565.835102	21.813607
80.116432	2572.348440	21.818624
80.395780	2550.595575	21.823642
80.192515	2565.178908	21.828659
80.458581	2566.103062	21.833677
80.129821	2564.563304	21.838695
80.014333	2564.520469	21.843712
80.357976	2579.831095	21.848730
80.249856	2592.393767	21.853747
80.535020	2583.045856	21.858765
80.366373	2590.642528	21.863783
80.741421	2609.260934	21.868800
81.150045	2607.954611	21.873818
80.842245	2624.108505	21.878835
81.503680	2607.785918	21.883853
81.711702	2614.501325	21.888871
81.691459	2608.776241	21.893888
81.878414	2604.818164	21.898906
81.785018	2611.182030	21.903923
82.363694	2617.680098	21.908941
82.329753	2598.570084	21.913959
81.775746	2580.647522	21.918976
82.223512	2573.958764	21.923994
81.897745	2568.517037	21.929011
81.743009	2561.576495	21.934029
81.820737	2597.724569	21.939047
81.753172	2597.973989	21.944064
81.946442	2594.179032	21.949082
82.151850	2603.420071	21.954099
82.146828	2596.647082	21.959117
82.134035	2615.208137	21.964135
82.537702	2618.546187	21.969152
82.619428	2622.316741	21.974170
82.721023	2633.152199	21.979187
82.948261	2629.739781	21.984205
82.697650	2641.395004	21.989223
82.528143	2636.253589	21.994240
83.196900	2611.717590	21.999258
82.997750	2633.302153	22.004275
82.926356	2625.313830	22.009293
83.063461	2643.125989	22.014311
83.186852	2653.801768	22.019328
83.605077	2656.463061	22.024346
83.250923	2657.973926	22.029363
83.591577	2660.754919	22.034381
83.613996	2658.827026	22.039399
83.630800	2652.644458	22.044416
83.661923	2653.162787	22.049434
83.541723	2680.035961	22.054451
84.013936	2679.547216	22.059469
83.896608	2681.649615	22.064487
84.249501	2680.087159	22.069504
84.549261	2676.392294	22.074522
84.462008	2688.283138	22.079539
84.718714	2667.504255	22.084557
84.714085	2667.473807	22.089575
84.516258	2662.324270	22.094592
84.840109	2657.066287	22.099610
84.730085	2674.583713	22.104627
84.945105	2662.565840	22.109645
85.074162	2668.167824	22.114663
85.267865	2699.777409	22.119680
84.760352	2698.975394	22.124698
84.906095	2704.820877	22.129715
84.963502	2705.398049	22.134733
84.988255	2704.559061	22.139751
85.120075	2708.687475	22.144768
85.284333	2718.705015	22.149786
85.438002	2735.833093	22.154803
85.514194	2725.335652	22.159821
85.733251	2727.145282	22.164839
85.796158	2737.895086	22.169856
86.205372	2732.522978	22.174874
86.005152	2731.955007	22.179891
86.286907	2742.942255	22.184909
86.216753	2746.153723	22.189927
86.561508	2747.354827	22.194944
86.641489	2738.298389	22.199962
86.676003	2752.663682	22.204979
86.946491	2738.446964	22.209997
86.724028	2744.299175	22.215015
86.724674	2751.111110	22.220032
86.631016	2732.982191	22.225050
86.749919	2737.697551	22.230067
86.730387	2741.741149	22.235085
86.743788	2750.765792	22.240103
86.509654	2763.292342	22.245120
87.074723	2770.969421	22.250138
87.197234	2779.791220	22.255155
87.187891	2766.802728	22.260173
87.284967	2779.224958	22.265191
87.096970	2805.280864	22.270208
87.576520	2786.990631	22.275226
87.397516	2798.145586	22.280243
87.437283	2807.741657	22.285261
87.609848	2828.309221	22.290279
87.852743	2829.739552	22.295296
88.081804	2825.170955	22.300314
88.106272	2831.146559	22.305331
88.243606	2825.647506	22.310349
88.425128	2826.582892	22.315367
88.455366	2853.808257	22.320384
89.028133	2838.185474	22.325402
89.584024	2837.286662	22.330419
89.429522	2819.928673	22.335437
89.302179	2808.483175	22.340455
89.245988	2801.065442	22.345472
89.475005	2797.842840	22.350490
89.300555	2806.400753	22.355507
89.597389	2810.663728	22.360525
89.915423	2799.875304	22.365543
89.459512	2805.102770	22.370560
89.532085	2802.964221	22.375578
89.444802	2797.347186	22.380595
89.041900	2806.653435	22.385613
89.645731	2807.622179	22.390631
89.377393	2800.973315	22.395648
89.447418	2806.684704	22.400666
89.425824	2824.220756	22.405683
89.678448	2831.814464	22.410701
89.704590	2832.063757	22.415719
89.553097	2846.839182	22.420736
89.873621	2865.780473	22.425754
90.103737	2866.476348	22.430771
90.377902	2875.893185	22.435789
90.738973	2878.711394	22.440807
90.307067	2890.797132	22.445824
90.980543	2889.310415	22.450842
91.068533	2894.284264	22.455859
91.141793	2898.923559	22.460877
91.302416	2888.611847	22.465895
91.058490	2889.643128	22.470912
91.252784	2877.133464	22.475930
91.239589	2875.882256	22.480947
91.664970	2884.483999	22.485965
91.518907	2883.371276	22.490983
91.272245	2889.504297	22.496000
91.697096	2921.563120	22.501018
91.784801	2919.153171	22.506035
91.830924	2927.417630	22.511053
91.669897	2915.314662	22.516071
91.897799	2929.898740	22.521088
92.003481	2913.333435	22.526106
92.500258	2927.033363	22.531123
92.419576	2941.725921	22.536141
92.683972	2934.838582	22.541159
92.601254	2939.533584	22.546176
92.787919	2939.064657	22.551194
92.700061	2937.985616	22.556211
92.710191	2937.769077	22.561229
92.834759	2944.596642	22.566247
92.992103	2946.595817	22.571264
93.246270	2936.702452	22.576282
93.165973	2940.920307	22.581299
93.024914	2952.964332	22.586317
93.189411	2956.569329	22.591335
93.362703	2969.342878	22.596352
93.695698	2964.774781	22.601370
93.674710	2979.477983	22.606387
93.772908	2975.210086	22.611405
93.797195	2957.052753	22.616423
93.688321	2965.161357	22.621440
94.050239	2974.204324	22.626458
94.247990	2980.393859	22.631475
94.211591	2994.995296	22.636493
94.177345	2993.411353	22.641511
94.049106	2993.209805	22.646528
94.068199	2997.279762	22.651546
94.394634	2992.760770	22.656563
94.418294	3013.204375	22.661581
94.857451	3021.526766	22.666599
94.854133	3024.773702	22.671616
94.880931	3013.341556	22.676634
95.175139	3013.939056	22.681651
94.800612	3013.257363	22.686669
94.920142	3014.001045	22.691687
94.727877	3028.005858	22.696704
95.166156	3036.861843	22.701722
95.220941	3037.109161	22.706739
95.375065	3045.265683	22.711757
95.678280	3042.110688	22.716775
95.671507	3039.264385	22.721792
96.010551	3052.180684	22.726810
96.239719	3062.463300	22.731827
96.307154	3069.389727	22.736845
96.629546	3057.282353	22.741863
96.902909	3055.485377	22.746880
96.491988	3044.847552	22.751898
96.660606	3015.569964	22.756915
96.487186	3028.620528	22.761933
96.602097	3056.306252	22.766951
96.659403	3054.808745	22.771968
96.665832	3061.157087	22.776986
96.592180	3059.131245	22.782003
96.669782	3061.980975	22.787021
96.808684	3070.709686	22.792039
96.816133	3093.220550	22.797056
96.939803	3092.480151	22.802074
97.353921	3092.641323	22.807091
97.266315	3106.971812	22.812109
97.326447	3113.637271	22.817127
97.601163	3126.066251	22.822144
97.355003	3136.211721	22.827162
97.452554	3130.373479	22.832179
97.647551	3139.944500	22.837197
97.841144	3138.559105	22.842215
98.006712	3149.164480	22.847232
98.133842	3140.789950	22.852250
98.495160	3133.047960	22.857267
98.563622	3152.938698	22.862285
98.871071	3162.680120	22.867303
99.065372	3166.287328	22.872320
99.080537	3162.111050	22.877338
99.206514	3155.005946	22.882355
99.689640	3148.738643	22.887373
99.537243	3149.075709	22.892391
99.526204	3124.773865	22.897408
99.409258	3120.538330	22.902426
99.878976	3118.630951	22.907443
99.684956	3112.791291	22.912461
99.556736	3116.383675	22.917479
99.609890	3134.739582	22.922496
99.808698	3153.855270	22.927514
99.949368	3139.645267	22.932531
100.138582	3141.549047	22.937549
100.046641	3139.152609	22.942567
100.343237	3142.527956	22.947584
99.958619	3136.217440	22.952602
100.561285	3141.083488	22.957619
100.501902	3147.430930	22.962637
100.550819	3154.817130	22.967655
100.576622	3172.812656	22.972672
100.397197	3176.926487	22.977690
100.523402	3171.233489	22.982707
100.561403	3187.020800	22.987725
100.811785	3204.099756	22.992743
100.883668	3198.386198	22.997760
100.915909	3199.609257	23.002778
101.527621	3199.548810	23.007795
101.488667	3203.502434	23.012813
101.594184	3199.958044	23.017831
102.078306	3206.231447	23.022848
101.825074	3223.092866	23.027866
102.366681	3225.871859	23.032883
102.255149	3217.737111	23.037901
102.116349	3187.737189	23.042919
102.302191	3207.038544	23.047936
102.266229	3205.979254	23.052954
102.328885	3214.885599	23.057971
101.688187	3212.859345	23.062989
101.868459	3209.008516	23.068007
102.563427	3227.039194	23.073024
102.577330	3240.729826	23.078042
102.809874	3243.996099	23.083059
102.595810	3253.204483	23.088077
102.905297	3246.946937	23.093095
103.257827	3259.714730	23.098112
103.198794	3276.698443	23.103130
103.313279	3271.375444	23.108147
103.547847	3280.351055	23.113165
103.414139	3277.576075	23.118183
103.860296	3278.517365	23.123200
103.708783	3286.125324	23.128218
103.721132	3283.823044	23.133235
103.530222	3305.972125	23.138253
103.597849	3308.464505	23.143271
103.976601	3305.755624	23.148288
104.102736	3316.286137	23.153306
104.630249	3322.082352	23.158323
104.980087	3329.999604	23.163341
105.249797	3325.782008	23.168359
105.299440	3314.678926	23.173376
105.183567	3321.415290	23.178394
105.719658	3316.452912	23.183411
105.583606	3309.248125	23.188429
105.467396	3292.723017	23.193447
105.528013	3282.063407	23.198464
105.183144	3290.497783	23.203482
105.425686	3295.692278	23.208499
105.889825	3305.455929	23.213517
105.987638	3312.311699	23.218535
105.770740	3306.822193	23.223552
105.647091	3313.692906	23.228570
105.816431	3326.731175	23.233587
106.150106	3313.988684	23.238605
105.879098	3328.737074	23.243623
106.430209	3339.951689	23.248640
106.120024	3338.431024	23.253658
106.351122	3343.736085	23.258675
106.539301	3349.611611	23.263693
106.470249	3345.716910	23.268711
106.535036	3360.969277	23.273728
106.429056	3376.010119	23.278746
107.028179	3364.739434	23.283763
107.378402	3377.825021	23.288781
107.760214	3393.947847	23.293799
107.901329	3388.487340	23.298816
107.930183	3383.035937	23.303834
107.630732	3372.107425	23.308851
108.007139	3385.411127	23.313869
108.017582	3385.677983	23.318887
108.456336	3374.082619	23.323904
108.328373	3395.144287	23.328922
108.653146	3393.025006	23.333939
108.371715	3389.255543	23.338957
108.405462	3390.911429	23.343975
108.655018	3388.836859	23.348992
108.184948	3387.518589	23.354010
108.541332	3371.329074	23.359027
108.202209	3381.258575	23.364045
108.220706	3404.424350	23.369063
108.362388	3409.911922	23.374080
108.531483	3417.262641	23.379098
108.771138	3435.295574	23.384115
109.224552	3445.687057	23.389133
109.192121	3447.253493	23.394151
109.376257	3447.292834	23.399168
109.320132	3461.144441	23.404186
109.599585	3463.395943	23.409203
110.133575	3468.179745	23.414221
110.182985	3469.078735	23.419239
110.911134	3456.992191	23.424256
110.722974	3478.633594	23.429274
110.803146	3468.982417	23.434291
110.532551	3454.693236	23.439309
110.568704	3453.820434	23.444327
110.755408	3459.225388	23.449344
110.800836	3457.542801	23.454362
110.828671	3452.519093	23.459379
111.019253	3460.346588	23.464397
110.874282	3455.320725	23.469415
111.021963	3448.691418	23.474432
110.911159	3472.951081	23.479450
111.224890	3473.368606	23.484467
111.115043	3488.679877	23.489485
110.914728	3499.218788	23.494503
111.185475	3494.240752	23.499520
111.002149	3511.108648	23.504538
111.567808	3524.718988	23.509555
112.013534	3529.698102	23.514573
112.353125	3532.901473	23.519591
112.631260	3527.583234	23.524608
113.147960	3527.943208	23.529626
113.048731	3527.323871	23.534643
112.836337	3537.812444	23.539661
113.022729	3528.377534	23.544679
113.012871	3516.960915	23.549696
112.708669	3521.356081	23.554714
113.084604	3524.540454	23.559731
113.293092	3533.004387	23.564749
113.461820	3545.547281	23.569767
113.655031	3551.947636	23.574784
113.178839	3551.109095	23.579802
113.360638	3561.876637	23.584819
113.492531	3553.004254	23.589837
113.614934	3582.762883	23.594855
113.593828	3577.698008	23.599872
113.432662	3588.431296	23.604890
113.885066	3593.192794	23.609907
114.134493	3605.207052	23.614925
113.920905	3613.034481	23.619943
114.218022	3615.657886	23.624960
114.327617	3636.262126	23.629978
114.723512	3626.283881	23.634995
115.434652	3629.467611	23.640013
115.263272	3635.569193	23.645031
115.752279	3615.673288	23.650048
115.884030	3615.794907	23.655066
116.131858	3632.151537	23.660083
115.858020	3616.539918	23.665101
115.798341	3615.189640	23.670119
116.292766	3613.254893	23.675136
116.217076	3625.792964	23.680154
116.117164	3619.504494	23.685171
115.976004	3616.675567	23.690189
116.078801	3624.285369	23.695207
116.320958	3620.036027	23.700224
116.525068	3626.364141	23.705242
116.176817	3616.272646	23.710259
116.573424	3628.677953	23.715277
116.652346	3643.582990	23.720295
116.632466	3651.818978	23.725312
116.675262	3655.562753	23.730330
116.767936	3650.429842	23.735347
117.281969	3659.478392	23.740365
117.173140	3677.867220	23.745383
117.336320	3687.971788	23.750400
117.380178	3689.787846	23.755418
117.102308	3686.663387	23.760435
117.252620	3692.809079	23.765453
117.191560	3712.220365	23.770471
117.542811	3703.038422	23.775488
117.700176	3730.250621	23.780506
117.847576	3739.533028	23.785523
118.289646	3733.960466	23.790541
118.181712	3742.537824	23.795559
118.596466	3763.515037	23.800576
118.646761	3767.225710	23.805594
118.979457	3750.101134	23.810611
119.131138	3758.323790	23.815629
119.118100	3765.925638	23.820647
119.291301	3747.127025	23.825664
119.399542	3757.184417	23.830682
119.312951	3777.780319	23.835699
119.991483	3781.731281	23.840717
120.118673	3776.002860	23.845735
120.346875	3776.311300	23.850752
120.419048	3792.510510	23.855770
120.443140	3782.308956	23.860787
121.098997	3775.148295	23.865805
120.591942	3767.425464	23.870823
120.814083	3745.963252	23.875840
120.479269	3755.710389	23.880858
120.348465	3772.129339	23.885875
120.750159	3764.394932	23.890893
120.556699	3773.626596	23.895911
120.739585	3776.855913	23.900928
121.065220	3797.082544	23.905946
120.960232	3783.640105	23.910963
121.434512	3798.846892	23.915981
121.297925	3803.922316	23.920999
121.418477	3796.764272	23.926016
121.662957	3825.545712	23.931034
121.560562	3826.205238	23.936051
121.886746	3816.243509	23.941069
122.161830	3826.420622	23.946087
122.411504	3847.654757	23.951104
122.415254	3852.160154	23.956122
121.989717	3861.336517	23.961139
122.442011	3851.459440	23.966157
122.638399	3846.999882	23.971175
122.530337	3862.308469	23.976192
122.745267	3879.060562	23.981210
122.917581	3882.034953	23.986227
123.059532	3881.070629	23.991245
123.269721	3891.445124	23.996263
123.211145	3903.419955	24.001280
123.310179	3903.973759	24.006298
123.722638	3912.012461	24.011315
123.976890	3913.389051	24.016333
123.898435	3912.239489	24.021351
124.040839	3927.185490	24.026368
124.230333	3945.460379	24.031386
123.916481	3943.541827	24.036403
124.295452	3938.017809	24.041421
124.286944	3940.830356	24.046439
124.439610	3949.163582	24.051456
124.751574	3963.946954	24.056474
124.300823	3967.595189	24.061491
124.631199	3965.810345	24.066509
124.758324	3974.865138	24.071527
124.786436	3982.190996	24.076544
125.576687	3998.495392	24.081562
125.176976	3996.613462	24.086579
125.679305	3991.042270	24.091597
125.886842	4013.897005	24.096615
126.137644	4012.685943	24.101632
126.238389	4014.161531	24.106650
126.477376	4016.331217	24.111667
126.644688	4011.733107	24.116685
126.503080	4017.388180	24.121703
126.845564	4012.900890	24.126720
126.992330	4009.273908	24.131738
126.799446	4016.344956	24.136755
127.098321	4005.010432	24.141773
127.070505	4007.236801	24.146791
126.998229	4016.989146	24.151808
127.295270	4033.006959	24.156826
127.135352	4050.765289	24.161843
127.459402	4048.839351	24.166861
127.349062	4051.957333	24.171879
127.800706	4054.416695	24.176896
128.084279	4063.556714	24.181914
127.621439	4077.848524	24.186931
128.044681	4073.715204	24.191949
128.300203	4081.634647	24.196967
128.082177	4104.936615	24.201984
128.427497	4092.486847	24.207002
128.750594	4106.051166	24.212019
129.232106	4096.771483	24.217037
128.963476	4104.989757	24.222055
128.631503	4112.961410	24.227072
129.342772	4118.751976	24.232090
129.006246	4129.950056	24.237107
129.027479	4124.083107	24.242125
129.147455	4139.825951	24.247143
129.629253	4157.561439	24.252160
129.940879	4158.669509	24.257178
129.851099	4157.441483	24.262195
130.336037	4172.655933	24.267213
130.215537	4192.122916	24.272231
130.167254	4189.933673	24.277248
130.433947	4175.666466	24.282266
130.420354	4184.906843	24.287283
130.564821	4208.862867	24.292301
130.993778	4214.433968	24.297319
131.041097	4209.415064	24.302336
131.343877	4219.939444	24.307354
131.154852	4221.634591	24.312371
131.463696	4229.037017	24.317389
131.506035	4243.212037	24.322407
131.510454	4246.704808	24.327424
132.102609	4236.870916	24.332442
131.658550	4243.116614	24.337459
132.251509	4262.545325	24.342477
132.307949	4262.696325	24.347495
132.269089	4269.049101	24.352512
132.667031	4265.288821	24.357530
132.417124	4275.928580	24.362547
132.454201	4267.278551	24.367565
132.730673	4282.562202	24.372583
133.059980	4299.975007	24.377600
133.077442	4292.003033	24.382618
133.283505	4298.594100	24.387635
133.437431	4283.329251	24.392653
133.636689	4294.008587	24.397671
133.367404	4302.092029	24.402688
133.721550	4306.445561	24.407706
133.673104	4321.577814	24.412723
133.932840	4323.604346	24.417741
133.958289	4323.956144	24.422759
134.120724	4328.831929	24.427776
134.740523	4338.246094	24.432794
134.379403	4353.181214	24.437811
134.529696	4349.645307	24.442829
134.589025	4348.611533	24.447847
135.072217	4356.759650	24.452864
135.325560	4360.337304	24.457882
135.185907	4369.562004	24.462899
135.222989	4358.831133	24.467917
135.610666	4365.047718	24.472935
135.575614	4366.588300	24.477952
135.952986	4369.429292	24.482970
135.990710	4381.983091	24.487987
136.320946	4382.039636	24.493005
136.360248	4387.096029	24.498023
136.298890	4379.979980	24.503040
136.639192	4368.458026	24.508058
136.545076	4387.038574	24.513075
137.091663	4399.995726	24.518093
137.225919	4408.155463	24.523111
137.021054	4406.871626	24.528128
137.445102	4406.021689	24.533146
137.267664	4416.320421	24.538163
137.230462	4395.106871	24.543181
137.509089	4413.838468	24.548199
137.617781	4431.209919	24.553216
137.834189	4430.114356	24.558234
137.595514	4434.098144	24.563251
138.293282	4448.912721	24.568269
138.383897	4449.150994	24.573287
138.178890	4460.846105	24.578304
138.520347	4456.514379	24.583322
138.277904	4466.843965	24.588339
138.854017	4471.459306	24.593357
138.735571	4476.313830	24.598375
138.406439	4497.186597	24.603392
139.106456	4500.140845	24.608410
139.110694	4519.067521	24.613427
138.985618	4526.628013	24.618445
139.635027	4526.154632	24.623463
139.609966	4545.109804	24.628480
139.958593	4551.463632	24.633498
139.996551	4556.641568	24.638515
140.204498	4556.721077	24.643533
140.756014	4571.165430	24.648551
140.607391	4573.069304	24.653568
140.585210	4582.395592	24.658586
140.502786	4588.843102	24.663603
140.769441	4590.456301	24.668621
141.044678	4598.376688	24.673639
140.767164	4612.207237	24.678656
140.876554	4616.715873	24.683674
141.252863	4630.122636	24.688691
141.444316	4638.918355	24.693709
141.559733	4646.901791	24.698727
141.598093	4649.557500	24.703744
142.006962	4664.701140	24.708762
141.858021	4675.542610	24.713779
142.107396	4666.636008	24.718797
142.819221	4661.936317	24.723815
142.986114	4664.061312	24.728832
142.928321	4658.242261	24.733850
143.327158	4667.685657	24.738867
143.373517	4671.148757	24.743885
143.622336	4676.333626	24.748903
143.082465	4686.150264	24.753920
143.608902	4680.038989	24.758938
143.514954	4685.593508	24.763955
143.530968	4694.339108	24.768973
143.833021	4681.265276	24.773991
143.785646	4698.919521	24.779008
144.077471	4713.152570	24.784026
144.269220	4716.718042	24.789043
144.433499	4715.143642	24.794061
144.778265	4718.106236	24.799079
144.269781	4735.260694	24.804096
144.513734	4752.768036	24.809114
144.883974	4745.380099	24.814131
144.842514	4749.445560	24.819149
145.396597	4761.459590	24.824167
145.592931	4769.729345	24.829184
145.453756	4775.024817	24.834202
145.727081	4767.981251	24.839219
145.698669	4785.629311	24.844237
145.805616	4788.895799	24.849255
145.852718	4793.468326	24.854272
145.809088	4805.767386	24.859290
146.251957	4815.692607	24.864307
146.819165	4818.680280	24.869325
146.554693	4825.982041	24.874343
146.653986	4844.677249	24.879360
146.772110	4849.683364	24.884378
147.159086	4852.374424	24.889395
147.194949	4871.263229	24.894413
147.915501	4857.842126	24.899431
148.084128	4877.614577	24.904448
148.578020	4869.131271	24.909466
148.302767	4875.049304	24.914483
148.232094	4881.721781	24.919501
148.411335	4866.899456	24.924519
148.786892	4867.109158	24.929536
148.581232	4855.837699	24.934554
148.585342	4866.501639	24.939571
148.512066	4902.811339	24.944589
148.680803	4892.893448	24.949607
148.902419	4895.420880	24.954624
149.311170	4914.919826	24.959642
149.256556	4926.943611	24.964659
149.544964	4933.123281	24.969677
149.959797	4942.611450	24.974695
150.186788	4967.158594	24.979712
150.278872	4954.808258	24.984730
150.334324	4959.338506	24.989747
150.351858	4971.687044	24.994765
150.524348	4963.585559	24.999783
150.769147	4963.547163	25.004800
150.650203	4979.359076	25.009818
151.128490	4982.082713	25.014835
150.922649	4989.591807	25.019853
151.214190	4991.986826	25.024871
151.178769	5000.622977	25.029888
151.428531	5008.067824	25.034906
151.787422	5017.581032	25.039923
151.564428	5016.286752	25.044941
151.913007	5034.561833	25.049959
152.358512	5041.155781	25.054976
152.697748	5030.658011	25.059994
153.096093	5031.466756	25.065011
152.720514	5029.948061	25.070029
152.856060	5026.916448	25.075047
152.963402	5032.624066	25.080064
153.321491	5033.621368	25.085082
153.370222	5021.523832	25.090099
153.208702	5024.278779	25.095117
153.393794	5048.160084	25.100135
153.579488	5067.617726	25.105152
153.692751	5059.566138	25.110170
154.119956	5054.795242	25.115187
153.770952	5085.943014	25.120205
154.052745	5085.239000	25.125223
154.450644	5097.100737	25.130240
154.249728	5093.473075	25.135258
154.496638	5113.385659	25.140275
154.754798	5129.657900	25.145293
154.749463	5125.586461	25.150311
154.810479	5132.063254	25.155328
155.056809	5153.333585	25.160346
155.521933	5148.569783	25.165363
155.460768	5158.387151	25.170381
156.080582	5165.664226	25.175399
156.046399	5182.480147	25.180416
156.307761	5181.616105	25.185434
156.577651	5167.831762	25.190451
156.538141	5181.227781	25.195469
156.805917	5180.222902	25.200487
156.704865	5184.240837	25.205504
156.714413	5192.570817	25.210522
157.048895	5191.205277	25.215539
156.695154	5202.868032	25.220557
157.370613	5206.280457	25.225575
157.204336	5217.672462	25.230592
157.411115	5228.811477	25.235610
157.933373	5230.536461	25.240627
157.538489	5250.749379	25.245645
157.827639	5249.122795	25.250663
158.307171	5270.260650	25.255680
158.263840	5281.145724	25.260698
158.758821	5271.535534	25.265715
158.687456	5285.951965	25.270733
159.016946	5292.155702	25.275751
159.640868	5301.528039	25.280768
159.565705	5304.621950	25.285786
159.622798	5306.670679	25.290803
159.483226	5306.646576	25.295821
159.570097	5321.990926	25.300839
159.766654	5338.407830	25.305856
159.980045	5337.617066	25.310874
160.483797	5353.348910	25.315891
160.465696	5365.427242	25.320909
160.639424	5362.489266	25.325927
160.627294	5365.200688	25.330944
160.828524	5372.304874	25.335962
161.193701	5378.548029	25.340979
161.412021	5389.126533	25.345997
161.384864	5393.858371	25.351015
161.611997	5386.613872	25.356032
161.648983	5396.624248	25.361050
161.951428	5404.870902	25.366067
161.876599	5412.085688	25.371085
162.207766	5416.236224	25.376103
162.369927	5420.293019	25.381120
162.627164	5435.429784	25.386138
162.923790	5448.504321	25.391155
162.580479	5449.613214	25.396173
162.756526	5447.634392	25.401191
163.350271	5440.663973	25.406208
163.048173	5461.045709	25.411226
163.330385	5457.815744	25.416243
163.350488	5479.362509	25.421261
163.577111	5480.396132	25.426279
163.675437	5486.049494	25.431296
163.382273	5501.193399	25.436314
164.136532	5522.353926	25.441331
164.361460	5530.427214	25.446349
164.289334	5541.844452	25.451367
164.461846	5550.171321	25.456384
164.212940	5553.956663	25.461402
164.590269	5554.887822	25.466419
165.002092	5573.145210	25.471437
164.955512	5597.089653	25.476455
165.305905	5607.870524	25.481472
165.316952	5612.654390	25.486490
165.825490	5632.332652	25.491507
165.843959	5638.958435	25.496525
166.289199	5641.063167	25.501543
166.380788	5646.712188	25.506560
166.716804	5663.479270	25.511578
166.887781	5650.354233	25.516595
167.031286	5649.007611	25.521613
166.934433	5668.042551	25.526631
167.069217	5673.843125	25.531648
167.372373	5681.027079	25.536666
167.445620	5684.939561	25.541683
167.559424	5710.557492	25.546701
167.800438	5710.066516	25.551719
168.149005	5714.048488	25.556736
167.763399	5731.021896	25.561754
168.221943	5738.035301	25.566771
168.510439	5746.525810	25.571789
168.330036	5761.908059	25.576807
168.821799	5765.837641	25.581824
168.986427	5781.967334	25.586842
168.732196	5788.703208	25.591859
169.442219	5795.364417	25.596877
169.478848	5800.173251	25.601895
169.639350	5812.022390	25.606912
169.789505	5826.300340	25.611930
170.286317	5833.757918	25.616947
170.132889	5839.550263	25.621965
170.307053	5850.332071	25.626983
171.051671	5859.015028	25.632000
170.487798	5854.946698	25.637018
170.957775	5871.145338	25.642035
170.979632	5886.366320	25.647053
171.091316	5889.025481	25.652071
171.609480	5897.817147	25.657088
171.650292	5927.093269	25.662106
171.587238	5918.057635	25.667123
172.060755	5930.015008	25.672141
171.717244	5944.167125	25.677159
172.241751	5947.022295	25.682176
172.081057	5961.745092	25.687194
172.622667	5975.879353	25.692212
172.827994	5979.669677	25.697229
172.874806	5989.322459	25.702247
173.246659	5999.378298	25.707264
173.474287	6006.092529	25.712282
173.640945	6014.524564	25.717300
173.609807	6016.825794	25.722317
173.677513	6034.884638	25.727335
174.139608	6049.472720	25.732352
173.809828	6052.709650	25.737370
174.112802	6054.442613	25.742388
174.225658	6076.558029	25.747405
174.145539	6077.413996	25.752423
174.804210	6080.831756	25.757440
175.005305	6110.513296	25.762458
175.269538	6103.908104	25.767476
175.420522	6102.572021	25.772493
175.783692	6124.835150	25.777511
175.825989	6121.696275	25.782528
175.830911	6126.823094	25.787546
176.284663	6132.034047	25.792564
176.448681	6128.827807	25.797581
176.240529	6152.083936	25.802599
176.663721	6159.704253	25.807616
176.644924	6154.479869	25.812634
176.941009	6158.835644	25.817652
177.405951	6172.316113	25.822669
177.432451	6179.386142	25.827687
177.578239	6177.945383	25.832704
177.518467	6185.161973	25.837722
177.911988	6199.913518	25.842740
178.134170	6199.565819	25.847757
177.902112	6210.835139	25.852775
178.624801	6220.712661	25.857792
178.415828	6235.630729	25.862810
178.730050	6244.117259	25.867828
178.705221	6252.978763	25.872845
179.070390	6251.154449	25.877863
179.359136	6260.571329	25.882880
179.823874	6269.742565	25.887898
180.313509	6278.704148	25.892916
180.321090	6281.078954	25.897933
180.042824	6292.759970	25.902951
180.532072	6295.125282	25.907968
180.575851	6295.649715	25.912986
180.508059	6291.392591	25.918004
180.754276	6310.821303	25.923021
180.696613	6326.812274	25.928039
181.176407	6316.847996	25.933056
181.065733	6347.873049	25.938074
181.726937	6340.631207	25.943092
182.052108	6343.071676	25.948109
182.278931	6346.714419	25.953127
182.718386	6349.669954	25.958144
183.009579	6359.221157	25.963162
182.926912	6365.688732	25.968180
182.926306	6356.364528	25.973197
182.974060	6361.880476	25.978215
183.098737	6351.251110	25.983232
183.179407	6367.551604	25.988250
183.195161	6374.941660	25.993268
183.699451	6380.390057	25.998285
183.498077	6389.372162	26.003303
184.051092	6393.465042	26.008320
183.835830	6406.888783	26.013338
183.980295	6428.372594	26.018356
184.179129	6435.318185	26.023373
184.405460	6442.106452	26.028391
184.352116	6457.457362	26.033408
184.485266	6478.526504	26.038426
184.599113	6484.626954	26.043444
184.980850	6507.521528	26.048461
184.664793	6518.347386	26.053479
185.180330	6540.441023	26.058496
185.331575	6558.676857	26.063514
185.842147	6570.898726	26.068532
186.129084	6561.844271	26.073549
186.097399	6584.446572	26.078567
186.984080	6597.636425	26.083584
187.008155	6601.519065	26.088602
187.094882	6607.209795	26.093620
187.525616	6608.233397	26.098637
187.467595	6615.027771	26.103655
187.690672	6614.140447	26.108672
188.010183	6640.181503	26.113690
187.828934	6634.945998	26.118708
187.934857	6642.678827	26.123725
187.917968	6650.204351	26.128743
188.502845	6657.285504	26.133760
188.540227	6667.504145	26.138778
188.697475	6662.123709	26.143796
188.927671	6681.581517	26.148813
189.158218	6697.475628	26.153831
189.375669	6682.608657	26.158848
189.850136	6708.368269	26.163866
189.512931	6715.945174	26.168884
190.397419	6713.011976	26.173901
190.614810	6722.023522	26.178919
190.971197	6728.275367	26.183936
190.620394	6736.976790	26.188954
190.498562	6747.547836	26.193972
190.771743	6751.684685	26.198989
191.106392	6774.272408	26.204007
191.289884	6764.569446	26.209024
191.799936	6780.160717	26.214042
191.757961	6781.637312	26.219060
191.892420	6791.313908	26.224077
192.169394	6796.731493	26.229095
192.347510	6802.838774	26.234112
192.478228	6821.537450	26.239130
192.430594	6829.671408	26.244148
192.930342	6831.506619	26.249165
192.846923	6861.614616	26.254183
193.198035	6854.475756	26.259200
193.483036	6871.042283	26.264218
193.597775	6891.125060	26.269236
193.936678	6899.773255	26.274253
193.821074	6903.457744	26.279271
194.435398	6917.674170	26.284288
194.742696	6909.081600	26.289306
194.643230	6918.164514	26.294324
195.087643	6925.152439	26.299341
194.904771	6946.309076	26.304359
195.467198	6949.449175	26.309376
195.537633	6947.265525	26.314394
195.256785	6966.972725	26.319412
195.839081	6968.583247	26.324429
196.275581	6984.851578	26.329447
196.163020	6991.903996	26.334464
196.440018	7003.841895	26.339482
196.355635	7013.059408	26.344500
196.850811	7005.557237	26.349517
196.796724	7028.416685	26.354535
197.225643	7024.086743	26.359552
197.453282	7029.238488	26.364570
197.390808	7057.460327	26.369588
197.992029	7051.322007	26.374605
197.745383	7069.966769	26.379623
198.334619	7079.275425	26.384640
198.341360	7081.329163	26.389658
198.400390	7087.167193	26.394676
198.855742	7096.912242	26.399693
199.445373	7113.929587	26.404711
199.209014	7122.572146	26.409728
199.571330	7119.709401	26.414746
199.600025	7136.231136	26.419764
199.610823	7148.740015	26.424781
199.630804	7141.427342	26.429799
199.680908	7162.389048	26.434816
199.996238	7170.055247	26.439834
200.344739	7184.615903	26.444852
200.967341	7190.318325	26.449869
201.103095	7207.463532	26.454887
201.070541	7216.851379	26.459904
201.578055	7199.296830	26.464922
201.391946	7222.315411	26.469940
201.704286	7243.777324	26.474957
201.432631	7243.793940	26.479975
201.634849	7263.205110	26.484992
201.870065	7271.732817	26.490010
201.917190	7285.076147	26.495028
202.397299	7301.226553	26.500045
202.773956	7309.532440	26.505063
203.124042	7330.959095	26.510080
203.140929	7334.081512	26.515098
203.328497	7351.908235	26.520116
203.435474	7367.478480	26.525133
203.642568	7371.524815	26.530151
204.309390	7382.084905	26.535168
204.823720	7379.122965	26.540186
204.396785	7395.532021	26.545204
205.053981	7401.684817	26.550221
205.394206	7408.685449	26.555239
205.383112	7412.537870	26.560256
205.828585	7407.905020	26.565274
205.893334	7418.812702	26.570292
206.027974	7430.627957	26.575309
206.127177	7449.518456	26.580327
206.121831	7443.065148	26.585344
206.412582	7451.911413	26.590362
206.421155	7474.019246	26.595380
206.718095	7469.656648	26.600397
206.890338	7493.147248	26.605415
207.199578	7500.323947	26.610432
207.395603	7519.232398	26.615450
207.471057	7536.432030	26.620468
207.673794	7534.475319	26.625485
208.218438	7552.171601	26.630503
208.108857	7575.611227	26.635520
208.858854	7573.049004	26.640538
208.677110	7591.838025	26.645556
208.884087	7606.127894	26.650573
209.140961	7609.476133	26.655591
209.137877	7617.316451	26.660608
209.473713	7632.734943	26.665626
209.417444	7650.274652	26.670644
209.663842	7658.480169	26.675661
209.565758	7672.002976	26.680679
209.880617	7696.856488	26.685696
210.567726	7718.387081	26.690714
210.650084	7721.935087	26.695732
210.464801	7730.597104	26.700749
211.005560	7753.075780	26.705767
211.190568	7768.568157	26.710784
211.345354	7779.242258	26.715802
211.362584	7801.643682	26.720820
211.559869	7815.298958	26.725837
211.716104	7828.726321	26.730855
212.114315	7855.496734	26.735872
212.714072	7851.656589	26.740890
213.143806	7872.017002	26.745908
213.517236	7875.830419	26.750925
213.695472	7875.403312	26.755943
214.082607	7883.200553	26.760960
214.295468	7876.133698	26.765978
214.329002	7890.437518	26.770996
214.496820	7900.848061	26.776013
214.827951	7916.866980	26.781031
214.687447	7903.017315	26.786048
214.869654	7905.995176	26.791066
214.924672	7904.032898	26.796084
215.410978	7935.119958	26.801101
215.701296	7930.597655	26.806119
215.578950	7932.340459	26.811136
215.907615	7958.646034	26.816154
215.994895	7972.941048	26.821172
216.088847	7965.791410	26.826189
216.342625	7985.980988	26.831207
216.780507	7998.640507	26.836224
216.754377	7995.098281	26.841242
216.864372	8017.607553	26.846260
217.005302	8021.342853	26.851277
217.237999	8041.224877	26.856295
217.268425	8056.566651	26.861312
217.722586	8076.017532	26.866330
218.066491	8094.406039	26.871348
218.188483	8114.224534	26.876365
218.082230	8120.799113	26.881383
218.242308	8147.414037	26.886400
218.899679	8155.940209	26.891418
219.512997	8185.873389	26.896436
219.555710	8185.154404	26.901453
219.966471	8201.399105	26.906471
220.069479	8227.313155	26.911488
220.075334	8221.130197	26.916506
220.377091	8231.699196	26.921524
220.431745	8244.819982	26.926541
220.649959	8262.385116	26.931559
221.147322	8268.282694	26.936576
221.430999	8276.232697	26.941594
221.670242	8306.163325	26.946612
221.670218	8305.535672	26.951629
222.365926	8314.591973	26.956647
222.236929	8337.581471	26.961664
222.654179	8342.567635	26.966682
222.987102	8342.326832	26.971700
223.271447	8368.269436	26.976717
223.431098	8364.883889	26.981735
223.268313	8375.360395	26.986752
223.845055	8375.317172	26.991770
223.835643	8395.141189	26.996788
223.795414	8397.790433	27.001805
224.302903	8413.427070	27.006823
224.460601	8430.565252	27.011840
224.676655	8438.957347	27.016858
224.648619	8462.570693	27.021876
225.127827	8468.851776	27.026893
225.296895	8479.141198	27.031911
225.274249	8494.906463	27.036928
225.956401	8514.945601	27.041946
225.942626	8516.310579	27.046964
226.331958	8521.780298	27.051981
227.021476	8533.219573	27.056999
227.176895	8536.410705	27.062016
227.398210	8537.795128	27.067034
227.734329	8553.323169	27.072052
227.807256	8556.962713	27.077069
228.367085	8564.367869	27.082087
228.292618	8570.991730	27.087104
228.548497	8563.118794	27.092122
228.380617	8560.232338	27.097140
228.677568	8586.729294	27.102157
229.174815	8584.694653	27.107175
228.962701	8587.196683	27.112192
229.299054	8601.096673	27.117210
229.665115	8620.761268	27.122228
229.438877	8619.594422	27.127245
229.607603	8622.905458	27.132263
229.313330	8653.929140	27.137280
229.836374	8659.754886	27.142298
230.263936	8682.836450	27.147316
230.363017	8700.978623	27.152333
230.871972	8720.013241	27.157351
230.389536	8737.548163	27.162368
230.863569	8746.105737	27.167386
231.135327	8774.375446	27.172404
231.208271	8791.564254	27.177421
231.902718	8804.348226	27.182439
231.970782	8831.806539	27.187456
232.578447	8852.018307	27.192474
232.616641	8855.276919	27.197492
232.976128	8880.761346	27.202509
233.345291	8892.064775	27.207527
233.211677	8906.550721	27.212544
233.496167	8916.972588	27.217562
234.080807	8945.573711	27.222580
233.628379	8956.586805	27.227597
234.273496	8968.603213	27.232615
234.424313	8979.895520	27.237632
234.763993	9000.748803	27.242650
235.085574	9009.425441	27.247668
235.105351	9024.940046	27.252685
235.739244	9029.541700	27.257703
236.196319	9057.589893	27.262720
236.359221	9060.953182	27.267738
236.539701	9068.980497	27.272756
236.555263	9093.597368	27.277773
237.118058	9097.192333	27.282791
237.433966	9113.034604	27.287808
237.671484	9118.790333	27.292826
237.797308	9133.625881	27.297844
237.822627	9151.603529	27.302861
237.977595	9155.654211	27.307879
238.218495	9165.069710	27.312896
238.408953	9194.228704	27.317914
238.845404	9198.288027	27.322932
238.867557	9219.467383	27.327949
239.191464	9234.531806	27.332967
238.830769	9252.799409	27.337984
239.651643	9271.597264	27.343002
239.990429	9277.215017	27.348020
239.604779	9307.262594	27.353037
239.971937	9320.828876	27.358055
240.520092	9346.464046	27.363072
241.041006	9363.714153	27.368090
241.313554	9370.534647	27.373108
241.529226	9393.433279	27.378125
241.988284	9403.172059	27.383143
242.078508	9406.004715	27.388160
242.225408	9409.829154	27.393178
242.277784	9428.330393	27.398196
242.220601	9449.156888	27.403213
242.940589	9457.485168	27.408231
242.997470	9477.303519	27.413248
243.388415	9484.381767	27.418266
243.690263	9492.643667	27.423284
244.034971	9513.890639	27.428301
244.705692	9504.580482	27.433319
244.747179	9524.891380	27.438336
244.679788	9532.918923	27.443354
245.197703	9538.285833	27.448372
244.881353	9542.201808	27.453389
245.244206	9560.072163	27.458407
245.646774	9571.105893	27.463424
245.918071	9575.042940	27.468442
246.148691	9589.033734	27.473460
246.082215	9607.012884	27.478477
246.493402	9608.981222	27.483495
246.677467	9633.630165	27.488512
246.650274	9639.356564	27.493530
246.807326	9653.514745	27.498548
246.926024	9680.116232	27.503565
247.169866	9700.584543	27.508583
247.560351	9729.772123	27.513600
247.574138	9744.626751	27.518618
248.231386	9760.063533	27.523636
248.346271	9773.281182	27.528653
248.593779	9793.788393	27.533671
248.953709	9816.420399	27.538688
248.859837	9834.706810	27.543706
249.360170	9863.220327	27.548724
249.351706	9876.497827	27.553741
249.892158	9890.537735	27.558759
250.286803	9917.425651	27.563776
250.681042	9936.624836	27.568794
251.301364	9935.850515	27.573812
251.583380	9958.052902	27.578829
251.858507	9964.346247	27.583847
251.981407	9972.610393	27.588864
252.373133	9977.260216	27.593882
252.748404	9988.319228	27.598900
252.802247	9988.154449	27.603917
253.217788	10000.638878	27.608935
253.396076	10009.141235	27.613952
253.333501	10022.482937	27.618970
253.730832	10025.193282	27.623988
253.763384	10040.361747	27.629005
254.458614	10059.928053	27.634023
254.281104	10076.063915	27.639040
254.305058	10083.179432	27.644058
254.967453	10103.953276	27.649076
255.193287	10115.794064	27.654093
255.184809	10126.856707	27.659111
255.406394	10143.220518	27.664128
255.533551	10167.396029	27.669146
255.784005	10177.546282	27.674164
256.065764	10201.428476	27.679181
256.395803	10221.148269	27.684199
256.665614	10236.146958	27.689216
256.686964	10256.151749	27.694234
257.058866	10263.706915	27.699252
257.166502	10300.375263	27.704269
257.503024	10318.420182	27.709287
257.783919	10339.144717	27.714304
257.786289	10361.877536	27.719322
258.123708	10375.529981	27.724340
258.351950	10397.143976	27.729357
258.774911	10425.396364	27.734375
259.367747	10440.281220	27.739392
259.584792	10463.532493	27.744410
260.244555	10481.299687	27.749428
260.235917	10493.244089	27.754445
260.661353	10495.396093	27.759463
261.045774	10503.479453	27.764480
260.995974	10531.797534	27.769498
261.476900	10539.308036	27.774516
261.458995	10554.272635	27.779533
261.797026	10568.927152	27.784551
262.036460	10571.196548	27.789568
262.022851	10601.531694	27.794586
262.447024	10603.208913	27.799604
262.601626	10623.020419	27.804621
263.113742	10634.704010	27.809639
263.264687	10647.602116	27.814656
262.801160	10666.209718	27.819674
263.424305	10686.138465	27.824692
263.694433	10700.994169	27.829709
264.232143	10728.683014	27.834727
264.373415	10742.982626	27.839744
264.278328	10767.889771	27.844762
264.518677	10773.090269	27.849780
264.775289	10800.282131	27.854797
265.019555	10829.413167	27.859815
265.588265	10835.050994	27.864832
266.106204	10862.841020	27.869850
266.836468	10875.400968	27.874868
266.947674	10892.298188	27.879885
267.345988	10898.837813	27.884903
267.762603	10918.854541	27.889920
267.714665	10921.670906	27.894938
268.256148	10916.832918	27.899956
268.679088	10942.281804	27.904973
268.809371	10951.037588	27.909991
269.102190	10951.968480	27.915008
268.906092	10980.274499	27.920026
269.446273	10981.567072	27.925044
269.351838	10991.269870	27.930061
269.483395	11023.010043	27.935079
269.950035	11027.609199	27.940096
270.030940	11050.174830	27.945114
269.949184	11065.259954	27.950132
270.240572	11099.825586	27.955149
270.655152	11110.959237	27.960167
271.231518	11143.996090	27.965184
271.285664	11173.406522	27.970202
271.925035	11177.425744	27.975220
272.356856	11195.661519	27.980237
272.542345	11210.693174	27.985255
272.840203	11218.693516	27.990272
272.889249	11245.772327	27.995290
273.350328	11246.513157	28.000308
273.890626	11260.906437	28.005325
274.108805	11273.845145	28.010343
274.144351	11285.922274	28.015360
274.660305	11308.295862	28.020378
274.755230	11310.581363	28.025396
275.008089	11331.187348	28.030413
275.142125	11340.973140	28.035431
275.598833	11353.616476	28.040448
275.431031	11377.849637	28.045466
276.030177	11391.251736	28.050484
276.241399	11416.971115	28.055501
276.672180	11433.288293	28.060519
277.165181	11437.107246	28.065536
277.122639	11460.651007	28.070554
277.399075	11477.962707	28.075572
277.903693	11494.689214	28.080589
277.919601	11505.057891	28.085607
277.924897	11522.242696	28.090624
278.342521	11544.606076	28.095642
278.741316	11561.798389	28.100660
279.124112	11577.199563	28.105677
279.102388	11588.047973	28.110695
279.683436	11613.558462	28.115712
279.338933	11637.829085	28.120730
279.946602	11651.915377	28.125748
280.399659	11666.917434	28.130765
280.233109	11684.294666	28.135783
280.828919	11697.986696	28.140800
280.920445	11724.911978	28.145818
281.016416	11739.353889	28.150836
281.493777	11771.041562	28.155853
281.706032	11792.652992	28.160871
282.089863	11796.274999	28.165888
281.693662	11830.827393	28.170906
282.387351	11853.868798	28.175924
282.603805	11872.155105	28.180941
283.047145	11906.043491	28.185959
283.306051	11920.223879	28.190976
283.324928	11948.934894	28.195994
283.910743	11976.350096	28.201012
284.269215	12004.986986	28.206029
284.218402	12032.596485	28.211047
284.837889	12059.149912	28.216064
285.035877	12077.467865	28.221082
285.397805	12086.018194	28.226100
286.323682	12098.292327	28.231117
286.517850	12111.059994	28.236135
286.926622	12125.785396	28.241152
286.815750	12134.822741	28.246170
287.325012	12162.446287	28.251188
287.589153	12181.163096	28.256205
288.032646	12194.236279	28.261223
288.279423	12205.244003	28.266240
288.439207	12216.923939	28.271258
288.944530	12233.113019	28.276276
289.182928	12255.060303	28.281293
289.280578	12264.728194	28.286311
289.843896	12284.414353	28.291328
290.267401	12295.358277	28.296346
290.383862	12308.153120	28.301364
290.955900	12322.298675	28.306381
291.014431	12332.301593	28.311399
291.043271	12342.405538	28.316416
291.342654	12360.605433	28.321434
291.386084	12392.689820	28.326452
291.687958	12400.566401	28.331469
292.116709	12437.272452	28.336487
292.329258	12453.187900	28.341504
292.732497	12462.901539	28.346522
292.913088	12489.543945	28.351540
293.283104	12520.685953	28.356557
293.272207	12536.532041	28.361575
293.876538	12555.913166	28.366592
294.180176	12572.306871	28.371610
294.408320	12581.688678	28.376628
295.195180	12592.708284	28.381645
295.450394	12631.519408	28.386663
295.240782	12633.457551	28.391680
295.623332	12652.485452	28.396698
295.937978	12681.753972	28.401716
296.478142	12699.180198	28.406733
296.735928	12707.581829	28.411751
296.900616	12727.818127	28.416768
297.389717	12757.763875	28.421786
297.379754	12773.632889	28.426804
297.668882	12784.066761	28.431821
297.869698	12816.812995	28.436839
298.316744	12827.261773	28.441856
298.849159	12846.057151	28.446874
299.058090	12867.468095	28.451892
299.642793	12882.597658	28.456909
299.315673	12895.805817	28.461927
299.835493	12898.866717	28.466944
300.191572	12926.390827	28.471962
300.075929	12948.714266	28.476980
300.299567	12960.783636	28.481997
300.471739	12989.334089	28.487015
300.980053	13021.654915	28.492032
300.849779	13029.884467	28.497050
301.094227	13064.735465	28.502068
302.026876	13092.601079	28.507085
301.872469	13109.280576	28.512103
302.194305	13117.771110	28.517120
302.612679	13156.345392	28.522138
302.695708	13185.145703	28.527156
303.245656	13192.892660	28.532173
303.600385	13232.538112	28.537191
303.937447	13261.254045	28.542208
304.080097	13279.110570	28.547226
304.345422	13305.501598	28.552244
304.791807	13333.911236	28.557261
304.946656	13365.233815	28.562279
305.490769	13372.887277	28.567296
306.024705	13406.347064	28.572314
306.260882	13432.976329	28.577332
306.806729	13445.197678	28.582349
306.981255	13482.492534	28.587367
307.265275	13496.219491	28.592384
307.827062	13511.291977	28.597402
308.160087	13538.630270	28.602420
308.815538	13551.887786	28.607437
308.439369	13586.669105	28.612455
308.871874	13589.322257	28.617472
309.315892	13602.327953	28.622490
309.353959	13630.726782	28.627508
309.774640	13647.942135	28.632525
310.236014	13666.285351	28.637543
310.692990	13693.688520	28.642560
311.335141	13705.388330	28.647578
311.650189	13704.223858	28.652596
312.427194	13732.215568	28.657613
312.025428	13738.515864	28.662631
312.427035	13750.934613	28.667648
312.882392	13768.500496	28.672666
312.745147	13779.290672	28.677684
313.019937	13800.468209	28.682701
313.094563	13826.833288	28.687719
313.364718	13843.692374	28.692736
314.034045	13875.255559	28.697754
314.196845	13902.693501	28.702772
314.688152	13918.354757	28.707789
314.808606	13954.362740	28.712807
315.240321	13964.146646	28.717824
315.730094	13985.172296	28.722842
315.535626	14016.364745	28.727860
315.813729	14040.677930	28.732877
316.071704	14061.938953	28.737895
316.151256	14084.997558	28.742912
316.759569	14114.450226	28.747930
317.256966	14139.746893	28.752948
317.384777	14146.876989	28.757965
318.380643	14179.267711	28.762983
318.711565	14201.199202	28.768000
319.051246	14207.145536	28.773018
318.901550	14237.591944	28.778036
319.380775	14254.008775	28.783053
319.765999	14258.368610	28.788071
320.127416	14279.152682	28.793088
320.761076	14307.925477	28.798106
320.886238	14314.121607	28.803124
321.238404	14326.079364	28.808141
321.376396	14344.947954	28.813159
321.546787	14354.825697	28.818176
321.897044	14365.683853	28.823194
322.048704	14387.010142	28.828212
322.861331	14406.476484	28.833229
322.921824	14417.518070	28.838247
323.325910	14447.789862	28.843264
323.492193	14460.861045	28.848282
323.383912	14483.510006	28.853300
323.793734	14505.252376	28.858317
324.165593	14527.481688	28.863335
324.333256	14550.444452	28.868352
324.549206	14579.326134	28.873370
324.693610	14612.127864	28.878388
325.164487	14639.780903	28.883405
325.308383	14684.056852	28.888423
325.633949	14708.534967	28.893440
326.265734	14726.602242	28.898458
326.344822	14771.620348	28.903476
326.951522	14790.634222	28.908493
326.960190	14819.653008	28.913511
327.214580	14855.001043	28.918528
327.931532	14883.671273	28.923546
328.098363	14910.297083	28.928564
328.687764	14935.562456	28.933581
328.729027	14979.737971	28.938599
329.464359	15012.203343	28.943616
329.676002	15032.444217	28.948634
329.775336	15058.291884	28.953652
330.286890	15089.840949	28.958669
330.941018	15103.000677	28.963687
331.227736	15134.432531	28.968704
331.437978	15153.764477	28.973722
331.642169	15182.584558	28.978740
332.224198	15216.962058	28.983757
332.527673	15232.594156	28.988775
332.924116	15268.092972	28.993792
333.850349	15281.991136	28.998810
333.879504	15291.632750	29.003828
334.404981	15316.803689	29.008845
334.811760	15324.666733	29.013863
335.134294	15343.702986	29.018880
335.806472	15355.107484	29.023898
336.091955	15382.831812	29.028916
336.505489	15385.258311	29.033933
336.443859	15396.008697	29.038951
336.673786	15424.189845	29.043968
337.075433	15436.802149	29.048986
337.211212	15462.239415	29.054004
337.094251	15489.240854	29.059021
337.433048	15509.686677	29.064039
337.665059	15540.624044	29.069056
338.102283	15559.569107	29.074074
338.292101	15598.037233	29.079092
338.599350	15620.590755	29.084109
338.584581	15660.835855	29.089127
338.775476	15704.224259	29.094144
339.296752	15736.263100	29.099162
339.366696	15769.265424	29.104180
340.095328	15807.641875	29.109197
340.468138	15836.636982	29.114215
341.008409	15864.510732	29.119232
341.799806	15884.013878	29.124250
342.089566	15915.820246	29.129268
342.326000	15939.588399	29.134285
343.056204	15952.594409	29.139303
343.256839	15981.873531	29.144320
343.659860	16000.416571	29.149338
343.746689	16028.929724	29.154356
344.228192	16032.899044	29.159373
344.243719	16056.320889	29.164391
344.135134	16092.355671	29.169408
344.695215	16108.767324	29.174426
344.705328	16154.613862	29.179444
345.264941	16181.325002	29.184461
345.594441	16211.568263	29.189479
345.646251	16247.444501	29.194496
346.348355	16277.963602	29.199514
346.296927	16304.090311	29.204532
346.387358	16343.285825	29.209549
347.202896	16381.215855	29.214567
347.327980	16418.240332	29.219584
347.953420	16449.405991	29.224602
348.791437	16479.174877	29.229620
348.505261	16507.536140	29.234637
349.262838	16537.272715	29.239655
349.479828	16571.344573	29.244672
349.883776	16609.757634	29.249690
350.010904	16647.523044	29.254708
350.467307	16664.305424	29.259725
351.475119	16695.841804	29.264743
351.782752	16730.316679	29.269760
352.219116	16741.515240	29.274778
352.569205	16763.595164	29.279796
353.257759	16788.325345	29.284813
353.737021	16803.401917	29.289831
353.857760	16819.215452	29.294848
354.249174	16855.065283	29.299866
354.535530	16863.623536	29.304884
355.049246	16882.589020	29.309901
355.094188	16900.754081	29.314919
355.194959	16940.431598	29.319936
355.534564	16957.793091	29.324954
355.889258	16988.246398	29.329972
356.075392	17022.904298	29.334989
357.045437	17039.651069	29.340007
357.267787	17063.700574	29.345024
357.548338	17087.292882	29.350042
358.076259	17107.600707	29.355060
358.254122	17135.777640	29.360077
358.440016	17166.169323	29.365095
358.487497	17201.742592	29.370112
359.358441	17218.297869	29.375130
359.620696	17258.751726	29.380148
359.645743	17289.805391	29.385165
360.179928	17310.859522	29.390183
360.245128	17347.232431	29.395200
360.863200	17377.972363	29.400218
361.312430	17413.977783	29.405236
361.703260	17444.509501	29.410253
362.226360	17461.117760	29.415271
362.457087	17490.222800	29.420288
362.728814	17519.050020	29.425306
362.856018	17558.314858	29.430324
363.148359	17583.395403	29.435341
363.778959	17601.882170	29.440359
363.990275	17639.628069	29.445376
364.497265	17665.634742	29.450394
364.892788	17692.263545	29.455412
365.071443	17738.271066	29.460429
365.709060	17758.602555	29.465447
365.846635	17790.787610	29.470464
366.127699	17811.230081	29.475482
366.649504	17846.119551	29.480500
367.003908	17884.401918	29.485517
367.693203	17907.943641	29.490535
368.255712	17944.292455	29.495552
368.459983	17956.286764	29.500570
368.969331	17971.231770	29.505588
369.018325	18008.515130	29.510605
369.400793	18022.979910	29.515623
369.618766	18040.744082	29.520640
370.311239	18071.792991	29.525658
370.680319	18091.366964	29.530676
370.833947	18113.619864	29.535693
371.796151	18130.553468	29.540711
372.095057	18151.623901	29.545728
372.200523	18161.514669	29.550746
372.401199	18180.563316	29.555764
372.656863	18216.813681	29.560781
372.871368	18252.943251	29.565799
372.960655	18270.569731	29.570816
373.139137	18297.356736	29.575834
373.685608	18339.177019	29.580852
373.893118	18379.833394	29.585869
374.640395	18405.382260	29.590887
375.142720	18442.982619	29.595904
375.369635	18476.454653	29.600922
375.801232	18502.482983	29.605940
376.132137	18537.567806	29.610957
376.911217	18562.408653	29.615975
377.557934	18588.040619	29.620992
378.168530	18623.017944	29.626010
378.431254	18642.833971	29.631028
378.820959	18654.679936	29.636045
379.122524	18679.412269	29.641063
379.300201	18711.586187	29.646080
379.240316	18731.975784	29.651098
379.864511	18751.632922	29.656116
379.828014	18792.042161	29.661133
380.141751	18819.271094	29.666151
380.476518	18856.189170	29.671168
380.489711	18898.980108	29.676186
381.252320	18937.303092	29.681204
381.564318	18975.322294	29.686221
382.303902	19015.616481	29.691239
382.368341	19061.150015	29.696256
382.585158	19102.906888	29.701274
383.109197	19127.782837	29.706292
383.770535	19176.528334	29.711309
383.878412	19219.696960	29.716327
384.487498	19249.488194	29.721344
384.662901	19293.266926	29.726362
385.414396	19323.208163	29.731380
385.774376	19353.746932	29.736397
386.261945	19391.544195	29.741415
386.371593	19427.077299	29.746432
386.924674	19454.157392	29.751450
387.354335	19486.842906	29.756468
387.491842	19528.591882	29.761485
388.101561	19567.674584	29.766503
388.441224	19605.830956	29.771520
388.713025	19636.373776	29.776538
389.401958	19673.550435	29.781556
389.553170	19709.722010	29.786573
390.483073	19741.403213	29.791591
390.682452	19779.871634	29.796608
390.623661	19818.737476	29.801626
391.343801	19840.289051	29.806644
391.543580	19882.310799	29.811661
392.293848	19905.049227	29.816679
392.526769	19938.252079	29.821696
392.679661	19978.115859	29.826714
393.436228	19999.310088	29.831732
393.560989	20029.693483	29.836749
393.967863	20058.255305	29.841767
394.513864	20087.152036	29.846784
394.534689	20112.311218	29.851802
394.995828	20152.635249	29.856820
395.153662	20184.536273	29.861837
395.339755	20226.682533	29.866855
395.911327	20265.271878	29.871872
396.454973	20303.501773	29.876890
397.196105	20337.239424	29.881908
397.114990	20379.879495	29.886925
397.468639	20399.912758	29.891943
398.076219	20450.286714	29.896960
398.346078	20490.189147	29.901978
399.052390	20510.369222	29.906996
399.103646	20558.789187	29.912013
399.747273	20598.989565	29.917031
400.050569	20622.918940	29.922048
400.086335	20666.519410	29.927066
400.756019	20702.249633	29.932084
401.492317	20734.232713	29.937101
402.153466	20768.038050	29.942119
402.979964	20789.473971	29.947136
403.367871	20816.920936	29.952154
404.048326	20851.535136	29.957172
404.698302	20865.523104	29.962189
404.630999	20893.305510	29.967207
405.121601	20910.611529	29.972224
405.524325	20937.993186	29.977242
405.768229	20971.369694	29.982260
405.749330	20996.301873	29.987277
406.217885	21024.320733	29.992295
406.429629	21055.596531	29.997312
406.894605	21104.386421	30.002330
407.146185	21120.220281	30.007348
407.432361	21158.923477	30.012365
407.687801	21198.161546	30.017383
408.256611	21247.716648	30.022400
408.493598	21288.063109	30.027418
408.909160	21326.696447	30.032436
409.342677	21377.926475	30.037453
409.598480	21418.698957	30.042471
410.231855	21456.273447	30.047488
410.592364	21508.316812	30.052506
411.132770	21532.990283	30.057524
411.581921	21588.836053	30.062541
411.703420	21641.289800	30.067559
412.015127	21673.130408	30.072576
412.544267	21720.316023	30.077594
413.301032	21748.384656	30.082612
413.708607	21795.942138	30.087629
413.963937	21837.601745	30.092647
414.825039	21881.988176	30.097664
414.595350	21912.997956	30.102682
415.163735	21958.438798	30.107700
415.626596	22005.199452	30.112717
416.134472	22033.309677	30.117735
416.634846	22084.139825	30.122752
416.813359	22129.661300	30.127770
417.514303	22162.412873	30.132788
417.834535	22196.222234	30.137805
417.966687	22241.496261	30.142823
418.543826	22272.094362	30.147840
418.769402	22328.476155	30.152858
419.266721	22374.995654	30.157876
419.708550	22410.320984	30.162893
419.917688	22454.047237	30.167911
421.080105	22478.666650	30.172928
421.596083	22520.264395	30.177946
422.188261	22553.353177	30.182964
422.336193	22584.636059	30.187981
422.580165	22617.311074	30.192999
423.005467	22639.324902	30.198016
423.303105	22673.974576	30.203034
423.313629	22718.428048	30.208052
424.083271	22754.718465	30.213069
424.383846	22793.553911	30.218087
425.028908	22827.580491	30.223104
425.366892	22873.520675	30.228122
425.637052	22911.604619	30.233140
426.153997	22936.413318	30.238157
426.721398	22980.373439	30.243175
427.074418	23019.364717	30.248192
427.170263	23068.826734	30.253210
428.030555	23092.968771	30.258228
428.403293	23146.210310	30.263245
428.529366	23186.163401	30.268263
429.276938	23220.922771	30.273280
429.502646	23265.140319	30.278298
430.010644	23303.524850	30.283316
430.628916	23346.843689	30.288333
430.466306	23379.617300	30.293351
431.266389	23421.315397	30.298368
431.586841	23476.734597	30.303386
432.268381	23512.128279	30.308404
432.696924	23548.935580	30.313421
433.028698	23599.036591	30.318439
433.894958	23642.479204	30.323456
433.959675	23685.239161	30.328474
434.302283	23709.816058	30.333492
435.023116	23758.112550	30.338509
435.158504	23802.985007	30.343527
435.768467	23845.174390	30.348544
435.987339	23893.371283	30.353562
436.646387	23922.424667	30.358580
437.386974	23964.468207	30.363597
437.286860	24026.601591	30.368615
437.799422	24060.666737	30.373632
438.368158	24115.298046	30.378650
438.841762	24144.287838	30.383668
439.318277	24192.690577	30.388685
439.425653	24248.358789	30.393703
439.977123	24280.398080	30.398720
440.414022	24331.275442	30.403738
440.395978	24377.133455	30.408756
441.249769	24427.220063	30.413773
441.375963	24475.960574	30.418791
442.096861	24523.568595	30.423808
442.708267	24570.168326	30.428826
442.775080	24621.910293	30.433844
443.279665	24668.889034	30.438861
443.780960	24717.978252	30.443879
444.613502	24769.911125	30.448896
445.011398	24816.594107	30.453914
445.480282	24837.737915	30.458932
446.109711	24889.665285	30.463949
446.231038	24939.391882	30.468967
447.228992	24972.866203	30.473984
447.303552	25031.579428	30.479002
447.842401	25060.241482	30.484020
448.129561	25109.401894	30.489037
448.301791	25152.672881	30.494055
449.085247	25191.880316	30.499072
449.396494	25238.603998	30.504090
450.119355	25276.257370	30.509108
450.841207	25315.445305	30.514125
451.518886	25361.930608	30.519143
451.911577	25375.436583	30.524160
452.505465	25403.549249	30.529178
453.243269	25426.257805	30.534196
453.321180	25458.476890	30.539213
453.878292	25485.398897	30.544231
454.416923	25504.830534	30.549248
454.501561	25541.087125	30.554266
454.648727	25571.502036	30.559284
455.360192	25592.562560	30.564301
455.225912	25637.702016	30.569319
455.956157	25668.366130	30.574336
456.196461	25718.032768	30.579354
456.466242	25763.489004	30.584372
457.082798	25803.330960	30.589389
457.481367	25847.283827	30.594407
458.226982	25883.935006	30.599424
458.608052	25924.825387	30.604442
458.943352	25967.432841	30.609460
459.454490	26021.031114	30.614477
459.700033	26062.448837	30.619495
460.101349	26104.329788	30.624512
460.538559	26148.267585	30.629530
461.103875	26203.251519	30.634548
461.643130	26251.354854	30.639565
461.499021	26312.978701	30.644583
462.238458	26351.344506	30.649600
462.803068	26416.362025	30.654618
463.200706	26478.855791	30.659636
464.121197	26518.090952	30.664653
464.237292	26566.817023	30.669671
465.100179	26610.032810	30.674688
465.543023	26645.297404	30.679706
465.994264	26691.025762	30.684724
466.639677	26738.368579	30.689741
466.779398	26783.120423	30.694759
467.563918	26823.731834	30.699776
468.015371	26868.826666	30.704794
468.366860	26909.803139	30.709812
468.943529	26966.336297	30.714829
469.131705	27014.108660	30.719847
469.900617	27061.116559	30.724864
470.191182	27110.140225	30.729882
470.496228	27151.613833	30.734900
471.072290	27195.648082	30.739917
471.235283	27258.233912	30.744935
471.707362	27299.118848	30.749952
472.193241	27360.513068	30.754970
472.692845	27406.229035	30.759988
473.424224	27451.127758	30.765005
473.881409	27508.672847	30.770023
474.586830	27561.247121	30.775040
475.210092	27611.504172	30.780058
475.546606	27661.281981	30.785076
476.220540	27697.292808	30.790093
476.631537	27740.081414	30.795111
477.156906	27772.208854	30.800128
477.820796	27826.645488	30.805146
478.278461	27872.770211	30.810164
478.988449	27898.145685	30.815181
479.417629	27938.660718	30.820199
479.372610	27988.934630	30.825216
480.124174	28021.365833	30.830234
480.366966	28066.684376	30.835252
481.231677	28102.153545	30.840269
481.929573	28147.469675	30.845287
482.082188	28181.984170	30.850304
482.927938	28216.929939	30.855322
483.370578	28249.062471	30.860340
484.086999	28276.238557	30.865357
484.561400	28300.871268	30.870375
485.099784	28326.591154	30.875392
485.517867	28365.714809	30.880410
485.425175	28399.945364	30.885428
486.074912	28430.302826	30.890445
486.574020	28451.572288	30.895463
486.609442	28497.664336	30.900480
486.889514	28525.852893	30.905498
487.339683	28573.141536	30.910516
487.792985	28620.000794	30.915533
487.783909	28681.061940	30.920551
488.383833	28725.339048	30.925568
488.714392	28784.824036	30.930586
489.151501	28848.550106	30.935604
489.605585	28899.510748	30.940621
489.837915	28958.946316	30.945639
490.485331	29025.792747	30.950656
491.224820	29073.240006	30.955674
491.627909	29130.149616	30.960692
492.236064	29188.845681	30.965709
492.834273	29250.940984	30.970727
492.771850	29306.792446	30.975744
493.797841	29356.439170	30.980762
494.223744	29422.771680	30.985780
494.813834	29475.430771	30.990797
495.256340	29538.843031	30.995815
495.797783	29591.488427	31.000832
496.677763	29653.526011	31.005850
497.089377	29696.742070	31.010868
497.725888	29744.652974	31.015885
497.743593	29816.956655	31.020903
498.543872	29862.550590	31.025920
499.641783	29900.682128	31.030938
499.834038	29956.089816	31.035956
500.537292	30003.968328	31.040973
501.021607	30058.116719	31.045991
501.354903	30097.665238	31.051008
502.067293	30147.066334	31.056026
502.386446	30213.804364	31.061044
503.274377	30238.582891	31.066061
503.401502	30295.759574	31.071079
503.785327	30346.240781	31.076096
504.480414	30391.487536	31.081114
505.021644	30454.101303	31.086132
505.333420	30496.521923	31.091149
506.072280	30548.866302	31.096167
506.483323	30597.463518	31.101184
507.016796	30648.971413	31.106202
506.918936	30707.170890	31.111220
507.736279	30771.443762	31.116237
508.443087	30815.112292	31.121255
509.108094	30867.580244	31.126272
509.683712	30917.621302	31.131290
509.862511	30968.806994	31.136308
510.206136	31005.371414	31.141325
510.440316	31071.170847	31.146343
510.984682	31124.747915	31.151360
511.581836	31187.913483	31.156378
511.799367	31260.868429	31.161396
512.487239	31319.340824	31.166413
512.725013	31383.859959	31.171431
513.465578	31446.952296	31.176448
514.340909	31514.265953	31.181466
514.703580	31581.806521	31.186484
515.169461	31622.368252	31.191501
515.629683	31689.258980	31.196519
516.087956	31736.072171	31.201536
516.710061	31769.781129	31.206554
516.817793	31840.526068	31.211572
517.286411	31901.901335	31.216589
518.005774	31947.886377	31.221607
519.034940	32001.767804	31.226624
519.807196	32054.795811	31.231642
520.075378	32105.891183	31.236660
520.882656	32158.487792	31.241677
521.456633	32197.805695	31.246695
521.709221	32254.299181	31.251712
522.479656	32291.392090	31.256730
522.568489	32345.994649	31.261748
523.079025	32385.153077	31.266765
523.348174	32449.828699	31.271783
523.858616	32514.565667	31.276800
524.646972	32554.912225	31.281818
524.984156	32630.077436	31.286836
525.627306	32676.900460	31.291853
526.114026	32742.721235	31.296871
526.170801	32803.672320	31.301888
526.663993	32861.450017	31.306906
527.334219	32930.762333	31.311924
528.443599	32974.691579	31.316941
529.118346	33031.086275	31.321959
529.580197	33087.737179	31.326976
530.691225	33134.310603	31.331994
531.199972	33192.055262	31.337012
531.549906	33233.529633	31.342029
532.426111	33289.756207	31.347047
532.994465	33336.858379	31.352064
533.626858	33370.436191	31.357082
533.985759	33427.925555	31.362100
534.191253	33483.342196	31.367117
534.681278	33526.920763	31.372135
535.179980	33583.109657	31.377152
535.458008	33634.046912	31.382170
535.729332	33684.105093	31.387188
536.287693	33757.884950	31.392205
536.791940	33817.677038	31.397223
536.833999	33889.097346	31.402240
537.590625	33951.063244	31.407258
537.929317	34028.789986	31.412276
538.661410	34094.023078	31.417293
539.239761	34160.566046	31.422311
539.378053	34239.431195	31.427328
540.478252	34295.478822	31.432346
541.206385	34354.891804	31.437364
541.651239	34425.673454	31.442381
542.318944	34491.546575	31.447399
542.773121	34552.046762	31.452416
543.249365	34606.948875	31.457434
543.873834	34686.669724	31.462452
544.376740	34754.612634	31.467469
545.062742	34809.578547	31.472487
545.233139	34873.566194	31.477504
545.990237	34923.841098	31.482522
546.745348	34993.450399	31.487540
546.885212	35057.948636	31.492557
547.384791	35125.508535	31.497575
547.660441	35191.603627	31.502592
548.327353	35272.156313	31.507610
549.028290	35343.076028	31.512628
549.487573	35407.708951	31.517645
550.414508	35476.815265	31.522663
550.720973	35544.383403	31.527680
551.336864	35601.954114	31.532698
551.970019	35671.605141	31.537716
552.164124	35739.041103	31.542733
552.774054	35793.972128	31.547751
553.513333	35864.423698	31.552768
554.153609	35918.819941	31.557786
554.892741	35977.665342	31.562804
554.918052	36046.957497	31.567821
555.817243	36106.313358	31.572839
556.592261	36166.633491	31.577856
557.153300	36214.555525	31.582874
557.542837	36278.190123	31.587892
558.150201	36332.081826	31.592909
558.805602	36387.269093	31.597927
559.239596	36453.787664	31.602944
559.701665	36521.766135	31.607962
560.225483	36589.463265	31.612980
560.545981	36663.319689	31.617997
561.406396	36716.839392	31.623015
561.549482	36790.400590	31.628032
562.041979	36859.325224	31.633050
562.677039	36930.959562	31.638068
563.211078	37007.344698	31.643085
563.712086	37084.821244	31.648103
564.396543	37153.939371	31.653120
565.207350	37220.897180	31.658138
565.726924	37303.853443	31.663156
565.837880	37379.385349	31.668173
566.399999	37450.361585	31.673191
567.374394	37522.431406	31.678208
568.020459	37585.264518	31.683226
568.732257	37668.184398	31.688244
569.015448	37746.438271	31.693261
569.788224	37808.654747	31.698279
569.966768	37886.746620	31.703296
570.551382	37969.903504	31.708314
571.531153	38031.947695	31.713332
571.782574	38116.905592	31.718349
572.538387	38193.164444	31.723367
573.130293	38264.489291	31.728384
573.798437	38340.627533	31.733402
574.351724	38415.431086	31.738420
574.641355	38487.624177	31.743437
575.580351	38557.245345	31.748455
576.629435	38637.522764	31.753472
577.292676	38700.312734	31.758490
578.172167	38767.473250	31.763508
578.633542	38830.192857	31.768525
579.342988	38891.151572	31.773543
579.293421	38954.864991	31.778560
579.431340	39022.685494	31.783578
580.234383	39096.248081	31.788596
580.701893	39166.482872	31.793613
581.490299	39244.950156	31.798631
581.912637	39322.831202	31.803648
582.633433	39389.818233	31.808666
583.329790	39471.757851	31.813684
583.410132	39541.695062	31.818701
584.426798	39597.245965	31.823719
585.283838	39689.683258	31.828736
586.293861	39741.394417	31.833754
587.000682	39804.465084	31.838772
587.555733	39858.587439	31.843789
588.595964	39906.635834	31.848807
589.038760	39981.713448	31.853824
589.481950	40031.871412	31.858842
590.162237	40089.240656	31.863860
590.791205	40164.682828	31.868877
591.303939	40202.292419	31.873895
591.717860	40266.565165	31.878912
592.103873	40328.636378	31.883930
592.978644	40370.750768	31.888948
592.766193	40417.539651	31.893965
593.438939	40478.194103	31.898983
594.187259	40550.767850	31.904000
593.984562	40612.059752	31.909018
594.418942	40683.590566	31.914036
594.934764	40766.948386	31.919053
595.562316	40842.166320	31.924071
595.935276	40917.950602	31.929088
596.434748	40996.962423	31.934106
597.337284	41070.017812	31.939124
598.015842	41152.144690	31.944141
598.632111	41230.554256	31.949159
599.095145	41312.461762	31.954176
599.648011	41394.446340	31.959194
600.637386	41462.059519	31.964212
600.921536	41560.563832	31.969229
601.966635	41616.094094	31.974247
602.491241	41700.104985	31.979264
603.347274	41783.660617	31.984282
603.731407	41846.867390	31.989300
604.172592	41922.054245	31.994317
605.181034	42009.793667	31.999335
605.795897	42087.017027	32.004352
606.177237	42162.148455	32.009370
606.756053	42245.344748	32.014388
607.287552	42319.577586	32.019405
608.268905	42396.539680	32.024423
608.951157	42477.304970	32.029440
609.183490	42560.563068	32.034458
609.580431	42623.912451	32.039476
610.088495	42724.065454	32.044493
610.794725	42809.964478	32.049511
611.435650	42890.946759	32.054528
612.428570	42972.508957	32.059546
612.971456	43045.685269	32.064564
613.392852	43116.327968	32.069581
614.058215	43202.232408	32.074599
614.707021	43305.866385	32.079616
615.160415	43377.489774	32.084634
615.890873	43463.365733	32.089652
616.336186	43561.162725	32.094669
617.024189	43638.550975	32.099687
617.547314	43724.888589	32.104704
618.275040	43814.921301	32.109722
619.117692	43896.319810	32.114740
619.300973	43993.107893	32.119757
620.237794	44070.598920	32.124775
620.796476	44154.615345	32.129792
621.507936	44251.232297	32.134810
622.365987	44330.132871	32.139828
622.887026	44407.176200	32.144845
623.583902	44480.449556	32.149863
623.916721	44575.391124	32.154880
624.925695	44654.198689	32.159898
625.549606	44734.323599	32.164916
625.937091	44823.432338	32.169933
626.773419	44904.874195	32.174951
627.373440	44988.556046	32.179968
627.981107	45064.817416	32.184986
628.702130	45145.556352	32.190004
628.955218	45229.593367	32.195021
630.026031	45314.313450	32.200039
630.695187	45400.186377	32.205056
631.107042	45486.484231	32.210074
632.118258	45566.608738	32.215092
632.565906	45642.377931	32.220109
633.207231	45712.814198	32.225127
633.599261	45789.625636	32.230144
633.822463	45871.419245	32.235162
634.814506	45936.923393	32.240180
635.130705	46018.032910	32.245197
635.952689	46097.594189	32.250215
636.475283	46184.199028	32.255232
637.053047	46268.689119	32.260250
637.405949	46354.381840	32.265268
637.929114	46439.008014	32.270285
638.924890	46520.986294	32.275303
639.491299	46592.603363	32.280320
640.390639	46684.171916	32.285338
641.109405	46770.661806	32.290356
641.593095	46858.292911	32.295373
642.833158	46934.340617	32.300391
643.855374	47019.363777	32.305408
644.037770	47088.737950	32.310426
644.705197	47156.835532	32.315444
645.615486	47226.898350	32.320461
646.110258	47308.808085	32.325479
646.804918	47388.642154	32.330496
647.076104	47472.042048	32.335514
648.037781	47539.021962	32.340532
648.734431	47620.817610	32.345549
648.982353	47707.935845	32.350567
649.664124	47787.950564	32.355584
650.471417	47873.082540	32.360602
651.181105	47950.987122	32.365620
651.957767	48034.037604	32.370637
652.799212	48113.225255	32.375655
653.107894	48196.180059	32.380672
653.390543	48285.123579	32.385690
654.314785	48379.266707	32.390708
655.146099	48462.619510	32.395725
655.560456	48546.354169	32.400743
656.340588	48628.342486	32.405760
656.905232	48715.700411	32.410778
657.777766	48785.765769	32.415796
658.550263	48884.622785	32.420813
659.285312	48973.627447	32.425831
660.057104	49043.947241	32.430848
660.483745	49143.671154	32.435866
661.021393	49219.446160	32.440884
661.771765	49306.065581	32.445901
662.451254	49392.826582	32.450919
663.143421	49485.677687	32.455936
663.811606	49562.360955	32.460954
664.609709	49635.915565	32.465972
665.159118	49723.511169	32.470989
666.131117	49810.402612	32.476007
666.676406	49885.357906	32.481024
667.163732	49975.134517	32.486042
667.753607	50057.946777	32.491060
668.615913	50142.801922	32.496077
668.833167	50221.210846	32.501095
670.102875	50303.741357	32.506112
670.382597	50396.532364	32.511130
671.450151	50476.219920	32.516148
672.017328	50567.672590	32.521165
672.557653	50645.859354	32.526183
673.482592	50737.203217	32.531200
674.389903	50812.835062	32.536218
674.371600	50884.568045	32.541236
675.183721	50963.383922	32.546253
675.951136	51062.392012	32.551271
676.668239	51147.496667	32.556288
677.074056	51240.422527	32.561306
677.424805	51318.002202	32.566324
678.330643	51397.022305	32.571341
678.150587	51483.442033	32.576359
679.130601	51570.163268	32.581376
679.752446	51658.084216	32.586394
680.710272	51741.133543	32.591412
681.305792	51840.451963	32.596429
681.819612	51941.878416	32.601447
682.808663	52022.147550	32.606464
683.508128	52095.759471	32.611482
684.529317	52184.030622	32.616500
685.130799	52285.867639	32.621517
685.776064	52375.329322	32.626535
686.044326	52461.038211	32.631552
686.502537	52558.200473	32.636570
687.300705	52659.697440	32.641588
688.050136	52760.110129	32.646605
688.379564	52839.613518	32.651623
689.274910	52958.006950	32.656640
689.687123	53050.264522	32.661658
690.617751	53148.678336	32.666676
691.447680	53241.316355	32.671693
691.882592	53350.590299	32.676711
693.019774	53446.861538	32.681728
693.761268	53552.137659	32.686746
694.662042	53643.622455	32.691764
695.505277	53741.592537	32.696781
695.915724	53832.710661	32.701799
696.770054	53935.177908	32.706816
697.594286	54034.896228	32.711834
698.277064	54124.928355	32.716852
699.171756	54214.780596	32.721869
699.764640	54313.723582	32.726887
700.165137	54404.883928	32.731904
700.710103	54521.032480	32.736922
701.329269	54611.228979	32.741940
701.745114	54717.253798	32.746957
702.378290	54834.109863	32.751975
703.328344	54924.505871	32.756992
704.191926	55041.363030	32.762010
704.850269	55143.963750	32.767028
706.036157	55238.485740	32.772045
706.666126	55331.564735	32.777063
707.795267	55424.972404	32.782080
708.509536	55527.092046	32.787098
709.306636	55614.692356	32.792116
710.086747	55718.912341	32.797133
710.498985	55804.498414	32.802151
711.153613	55905.884340	32.807168
712.259066	56003.525493	32.812186
712.525093	56088.536723	32.817204
713.558593	56185.514618	32.822221
714.029964	56289.618020	32.827239
714.771425	56369.800633	32.832256
715.510565	56478.650058	32.837274
716.270150	56562.773081	32.842292
716.924326	56655.753248	32.847309
717.251762	56771.047496	32.852327
718.345134	56864.960743	32.857344
718.774688	56965.504705	32.862362
719.735284	57046.810155	32.867380
720.396188	57158.608020	32.872397
720.950547	57267.207968	32.877415
721.729522	57352.102012	32.882432
722.416192	57468.276143	32.887450
722.926126	57570.048346	32.892468
723.711149	57665.652843	32.897485
724.314287	57771.953818	32.902503
725.272372	57872.010695	32.907520
725.450635	57975.526852	32.912538
726.302887	58058.497227	32.917556
727.089328	58155.184360	32.922573
727.876441	58253.419974	32.927591
728.649267	58348.006110	32.932608
729.291771	58457.634306	32.937626
729.767281	58559.549953	32.942644
730.670644	58652.403539	32.947661
731.300707	58755.109811	32.952679
731.750885	58865.467100	32.957696
732.273813	58985.241073	32.962714
733.349238	59092.254665	32.967732
734.278775	59191.128565	32.972749
734.909928	59307.903954	32.977767
735.674768	59412.082674	32.982784
736.725066	59509.314162	32.987802
737.379187	59615.970420	32.992820
738.437882	59720.519291	32.997837
738.705978	59824.257682	33.002855
739.855978	59928.223816	33.007872
740.692126	60031.711485	33.012890
741.147419	60132.924383	33.017908
742.064149	60235.097985	33.022925
742.731456	60357.049170	33.027943
743.503528	60449.850617	33.032960
744.350928	60565.472727	33.037978
745.075982	60689.482895	33.042996
745.461103	60782.994379	33.048013
745.896348	60906.276419	33.053031
746.782572	61004.420674	33.058048
747.566737	61122.660149	33.063066
748.255388	61248.992799	33.068084
749.005438	61357.904932	33.073101
749.716923	61476.720945	33.078119
751.045034	61583.895667	33.083136
751.990509	61692.745730	33.088154
752.683672	61792.410878	33.093172
753.643416	61909.450440	33.098189
754.622269	62016.286965	33.103207
755.516605	62099.494611	33.108224
756.595446	62210.392093	33.113242
756.961116	62310.196027	33.118260
758.149450	62401.781105	33.123277
758.349092	62515.271343	33.128295
759.229015	62606.573304	33.133312
760.075463	62706.634759	33.138330
761.092733	62809.310380	33.143348
761.572812	62903.504871	33.148365
762.159881	63011.643786	33.153383
763.151196	63118.585170	33.158400
763.896816	63224.872440	33.163418
764.751798	63319.891802	33.168436
765.531562	63409.380968	33.173453
766.149725	63532.427516	33.178471
766.678076	63625.435427	33.183488
767.887207	63717.022983	33.188506
768.419004	63821.319760	33.193524
769.110661	63917.456012	33.198541
769.481795	64036.905698	33.203559
770.399472	64147.517969	33.208576
771.266288	64254.460566	33.213594
771.741362	64377.276663	33.218612
772.445319	64480.751943	33.223629
772.756522	64598.584022	33.228647
773.585928	64714.169462	33.233664
774.375912	64834.863038	33.238682
774.617548	64955.736366	33.243700
775.478634	65075.724307	33.248717
776.515848	65187.270577	33.253735
777.263654	65293.713581	33.258752
778.667698	65406.034838	33.263770
779.178465	65512.296874	33.268788
779.784037	65618.625974	33.273805
780.361565	65739.732873	33.278823
781.249499	65848.089877	33.283840
782.056234	65957.244693	33.288858
782.577610	66087.503438	33.293876
783.143941	66201.882705	33.298893
783.760449	66329.636656	33.303911
784.199904	66450.732579	33.308928
785.238305	66583.481871	33.313946
785.640180	66732.526462	33.318964
786.623875	66849.406899	33.323981
787.437711	66989.503554	33.328999
788.448897	67135.966038	33.334016
789.279094	67253.051092	33.339034
790.030799	67396.302601	33.344052
790.749768	67522.030325	33.349069
791.711224	67651.107233	33.354087
792.600637	67782.643376	33.359104
793.544567	67916.504106	33.364122
794.346845	68041.645908	33.369140
795.676366	68162.655361	33.374157
796.467416	68293.610373	33.379175
797.280487	68413.960566	33.384192
798.539230	68540.983471	33.389210
798.823163	68670.747523	33.394228
799.429869	68801.761432	33.399245
800.269621	68927.376485	33.404263
800.905031	69063.457653	33.409280
801.525989	69198.208093	33.414298
801.904708	69329.376730	33.419316
802.849237	69466.907836	33.424333
803.708542	69608.272616	33.429351
804.586769	69750.779571	33.434368
805.630382	69877.934576	33.439386
806.361082	70028.788099	33.444404
807.600692	70155.754347	33.449421
808.490890	70286.888719	33.454439
809.152395	70424.991238	33.459456
810.334467	70540.942677	33.464474
810.899804	70673.821228	33.469492
811.913188	70805.823641	33.474509
812.628277	70945.766930	33.479527
813.180188	71076.728096	33.484544
814.107687	71195.785379	33.489562
815.050819	71330.104155	33.494580
816.147286	71458.050253	33.499597
817.272161	71583.349437	33.504615
818.099793	71711.139112	33.509632
818.969957	71833.143285	33.514650
819.605132	71958.171441	33.519668
820.596851	72071.007437	33.524685
821.486067	72201.344400	33.529703
822.278792	72326.291782	33.534720
822.954918	72439.453727	33.539738
823.561170	72569.871272	33.544756
824.565540	72694.027058	33.549773
825.871255	72804.393252	33.554791
826.649057	72934.999679	33.559808
827.129995	73048.260296	33.564826
827.440132	73180.248049	33.569844
828.761489	73306.214113	33.574861
829.498194	73428.919681	33.579879
830.229641	73557.514020	33.584896
830.980166	73663.619385	33.589914
831.521137	73788.509328	33.594932
832.419227	73901.977459	33.599949
832.995218	74029.265988	33.604967
833.506599	74152.847598	33.609984
834.807773	74275.818894	33.615002
835.547125	74411.708277	33.620020
836.418518	74525.437035	33.625037
837.328071	74650.909794	33.630055
838.273081	74774.113472	33.635072
839.434854	74887.030988	33.640090
840.421839	75011.885950	33.645108
841.304271	75138.580203	33.650125
842.278868	75257.702765	33.655143
842.731034	75368.159749	33.660160
843.520452	75484.348146	33.665178
844.645588	75611.966337	33.670196
845.408696	75728.767496	33.675213
846.282939	75858.458612	33.680231
847.232888	75986.607532	33.685248
847.944253	76117.876519	33.690266
848.393899	76240.835096	33.695284
849.247379	76382.137852	33.700301
850.094567	76505.734275	33.705319
850.868546	76633.675710	33.710336
852.190585	76761.483124	33.715354
852.927643	76898.899917	33.720372
853.771674	77017.535013	33.725389
854.728219	77143.855492	33.730407
855.565565	77286.418994	33.735424
856.682428	77403.948588	33.740442
857.133905	77542.289353	33.745460
857.970293	77673.502715	33.750477
859.449258	77809.999447	33.755495
859.507796	77944.638057	33.760512
860.663092	78067.774937	33.765530
861.211137	78218.506986	33.770548
862.244500	78353.297037	33.775565
863.079504	78486.653271	33.780583
863.460959	78632.058405	33.785600
864.372519	78777.345335	33.790618
864.733561	78928.119406	33.795636
865.601656	79070.107411	33.800653
866.811796	79224.430831	33.805671
867.752574	79375.251358	33.810688
868.896839	79517.683657	33.815706
869.842436	79671.161992	33.820724
870.745791	79812.510051	33.825741
871.774690	79946.070723	33.830759
872.677441	80103.740172	33.835776
873.570701	80231.556173	33.840794
874.339292	80370.576943	33.845812
875.311007	80519.160859	33.850829
876.168170	80657.770277	33.855847
876.393019	80804.948617	33.860864
877.716568	80960.865673	33.865882
878.924197	81098.945521	33.870900
879.579491	81230.526007	33.875917
880.816402	81376.282155	33.880935
881.183465	81527.142307	33.885952
882.391026	81674.746041	33.890970
883.447995	81817.839941	33.895988
884.211046	81960.926345	33.901005
884.922036	82100.176060	33.906023
885.391260	82251.049475	33.911040
886.392411	82396.667679	33.916058
887.400576	82556.519376	33.921076
887.966263	82701.686373	33.926093
889.010076	82825.658578	33.931111
889.829496	82970.836009	33.936128
890.647872	83118.083223	33.941146
891.198564	83258.176266	33.946164
891.581786	83414.018759	33.951181
892.874664	83560.500913	33.956199
893.288091	83733.592635	33.961216
894.396639	83870.883291	33.966234
895.478556	84025.608684	33.971252
896.252976	84184.675294	33.976269
897.615147	84326.753967	33.981287
897.972734	84489.080114	33.986304
898.977080	84644.499442	33.991322
899.649236	84802.941902	33.996340
900.472155	84969.686581	34.001357
901.456619	85131.768243	34.006375
902.415027	85296.702432	34.011392
903.321807	85458.584106	34.016410
904.190779	85631.020174	34.021428
904.790223	85811.727123	34.026445
905.617385	85971.208621	34.031463
906.501904	86159.874923	34.036480
907.702609	86329.566082	34.041498
908.865061	86501.833634	34.046516
909.757421	86675.684577	34.051533
910.906474	86845.590507	34.056551
911.844400	87008.224480	34.061568
912.728034	87173.197023	34.066586
913.605490	87351.307462	34.071604
914.640404	87533.854123	34.076621
915.519509	87688.960218	34.081639
915.983822	87869.648514	34.086656
917.107377	88045.312808	34.091674
918.124936	88215.389623	34.096692
918.889405	88395.336369	34.101709
920.065668	88577.121154	34.106727
921.091387	88736.069892	34.111744
922.329268	88914.638924	34.116762
923.514081	89085.675237	34.121780
924.057749	89256.495925	34.126797
925.137208	89420.654621	34.131815
925.874022	89603.836101	34.136832
926.620586	89779.385739	34.141850
927.720009	89939.703605	34.146868
928.422206	90120.192691	34.151885
929.611683	90293.059475	34.156903
930.388221	90476.544892	34.161920
931.344302	90646.022867	34.166938
932.291659	90810.447143	34.171956
932.721932	90993.253297	34.176973
933.934359	91168.685650	34.181991
935.069319	91354.865193	34.187008
935.983894	91531.311317	34.192026
937.020868	91713.630441	34.197044
938.308462	91897.187957	34.202061
939.347725	92063.073919	34.207079
939.872540	92249.089018	34.212096
940.841965	92414.482640	34.217114
941.732734	92581.991549	34.222132
942.705503	92764.227989	34.227149
943.711484	92945.308461	34.232167
944.802675	93120.781432	34.237184
945.384018	93300.567625	34.242202
946.476361	93481.131535	34.247220
947.925199	93645.916475	34.252237
948.833536	93818.228505	34.257255
949.923853	93993.480097	34.262272
950.595319	94149.497984	34.267290
951.604298	94310.803042	34.272308
952.351284	94488.893437	34.277325
953.375078	94636.191454	34.282343
954.147510	94812.229302	34.287360
954.963764	94984.185027	34.292378
955.924858	95136.534646	34.297396
956.586852	95316.651555	34.302413
957.632986	95490.693276	34.307431
958.341599	95673.564801	34.312448
959.281733	95846.158075	34.317466
959.968064	96021.022521	34.322484
961.071280	96211.504500	34.327501
961.657506	96387.609719	34.332519
962.600523	96583.938111	34.337536
963.403295	96782.253487	34.342554
964.604460	96965.034289	34.347572
965.677042	97158.921488	34.352589
967.161193	97346.437533	34.357607
968.377223	97532.726915	34.362624
969.203552	97718.176828	34.367642
970.557847	97889.646206	34.372660
971.209539	98081.229953	34.377677
972.212502	98268.794423	34.382695
973.330274	98446.428064	34.387712
974.357889	98616.633344	34.392730
975.734742	98817.035161	34.397748
976.284043	99007.079303	34.402765
977.487649	99174.372630	34.407783
977.893385	99369.811492	34.412800
978.955942	99561.553980	34.417818
979.997108	99753.155856	34.422836
980.690485	99949.184795	34.427853
981.655709	100139.972830	34.432871
982.239580	100345.050572	34.437888
983.404830	100553.452651	34.442906
984.194464	100765.362473	34.447924
985.037262	100957.765947	34.452941
986.346961	101179.222746	34.457959
987.445816	101380.393582	34.462976
988.259905	101583.119828	34.467994
989.372741	101797.700945	34.473012
990.055565	102008.188923	34.478029
990.746148	102216.391767	34.483047
992.002847	102432.568940	34.488064
992.856631	102642.489418	34.493082
994.206435	102848.372584	34.498100
995.260763	103066.969131	34.503117
996.265378	103269.297389	34.508135
997.884123	103481.485414	34.513152
998.343136	103692.404049	34.518170
999.894487	103906.550509	34.523188
1000.764458	104101.968005	34.528205
1001.882225	104289.494664	34.533223
1003.013899	104507.945015	34.538240
1003.759177	104709.105316	34.543258
1004.964665	104907.107547	34.548276
1005.930170	105122.994412	34.553293
1007.092607	105313.174185	34.558311
1008.350159	105510.627854	34.563328
1009.255936	105726.478918	34.568346
1010.718228	105919.469389	34.573364
1011.893885	106104.036100	34.578381
1013.205775	106289.658104	34.583399
1014.386564	106477.709341	34.588416
1014.792112	106661.989184	34.593434
1016.183756	106850.514864	34.598452
1016.832259	107036.682265	34.603469
1017.639467	107227.637466	34.608487
1018.685797	107407.358658	34.613504
1019.152384	107598.334775	34.618522
1020.343662	107770.169445	34.623540
1021.376166	107962.523924	34.628557
1022.489475	108145.418060	34.633575
1023.649593	108335.943022	34.638592
1024.079501	108541.687289	34.643610
1025.084971	108733.405861	34.648628
1025.799385	108932.254032	34.653645
1026.708573	109136.213874	34.658663
1027.571942	109333.064557	34.663680
1028.716137	109540.560485	34.668698
1029.808156	109741.036910	34.673716
1030.385041	109959.357976	34.678733
1031.606940	110169.100526	34.683751
1032.579678	110386.346392	34.688768
1033.230783	110615.389017	34.693786
1034.371526	110822.249397	34.698804
1035.166086	111051.702701	34.703821
1036.111628	111283.957735	34.708839
1037.671038	111500.229005	34.713856
1038.402649	111726.721663	34.718874
1040.019703	111946.356411	34.723892
1040.958330	112184.003829	34.728909
1041.874801	112406.608086	34.733927
1043.043624	112636.823671	34.738944
1043.801829	112860.699163	34.743962
1044.738969	113090.690787	34.748980
1046.254045	113325.250686	34.753997
1046.784999	113556.630716	34.759015
1048.073815	113786.443415	34.764032
1049.479777	114024.536326	34.769050
1050.630525	114233.929149	34.774068
1052.044365	114465.259708	34.779085
1053.040219	114694.241526	34.784103
1054.521586	114915.733969	34.789120
1055.767499	115140.522893	34.794138
1057.246950	115350.515971	34.799156
1058.440420	115550.321410	34.804173
1059.818523	115754.544595	34.809191
1060.966092	115967.675653	34.814208
1061.572785	116177.641656	34.819226
1062.758567	116373.020038	34.824244
1064.230324	116586.913109	34.829261
1064.853751	116795.461998	34.834279
1066.000104	117008.651826	34.839296
1066.770948	117221.601185	34.844314
1067.663477	117427.297662	34.849332
1068.477088	117643.435895	34.854349
1069.678237	117864.009607	34.859367
1070.630780	118079.038610	34.864384
1071.426476	118301.241056	34.869402
1072.668628	118515.262616	34.874420
1073.749514	118732.885420	34.879437
1074.788918	118956.953278	34.884455
1076.184457	119170.789710	34.889472
1077.275911	119406.306592	34.894490
1078.212091	119626.063383	34.899508
1079.034131	119839.479973	34.904525
1080.088586	120064.960442	34.909543
1081.152826	120288.388363	34.914560
1082.325135	120512.775841	34.919578
1083.232024	120743.417741	34.924596
1084.450878	120965.849686	34.929613
1085.618374	121193.398368	34.934631
1086.874940	121412.735696	34.939648
1087.811027	121654.644923	34.944666
1089.118720	121861.559068	34.949684
1089.999255	122067.911608	34.954701
1090.947730	122287.952628	34.959719
1092.224581	122492.037831	34.964736
1092.910890	122713.709310	34.969754
1094.326084	122922.032457	34.974772
1095.701912	123134.317300	34.979789
1096.108705	123355.330105	34.984807
1097.202104	123570.642695	34.989824
1097.781455	123789.146465	34.994842
1099.552502	123998.558980	34.999860
1100.524443	124241.421305	35.004877
1101.393279	124469.462825	35.009895
1102.841253	124688.286029	35.014912
1103.610127	124929.185168	35.019930
1104.312785	125168.398988	35.024948
1105.694044	125396.122200	35.029965
1106.750471	125639.070646	35.034983
1108.468624	125855.424512	35.040000
1109.343537	126105.883967	35.045018
1110.519202	126339.592109	35.050036
1111.635688	126572.031789	35.055053
1112.236210	126820.286549	35.060071
1113.988608	127051.801140	35.065088
1114.683051	127290.222006	35.070106
1115.803956	127534.962059	35.075124
1116.866504	127771.323422	35.080141
1117.359307	128020.353519	35.085159
1118.522914	128282.709722	35.090176
1119.656140	128543.590271	35.095194
1120.627460	128793.472884	35.100212
1122.171276	129055.227911	35.105229
1123.374362	129312.339062	35.110247
1124.481245	129565.589716	35.115264
1125.855877	129819.546066	35.120282
1127.105473	130085.553800	35.125300
1128.316771	130336.790845	35.130317
1129.441646	130586.041484	35.135335
1130.756323	130838.989349	35.140352
1131.597903	131107.582881	35.145370
1132.992576	131348.061628	35.150388
1134.383963	131596.667888	35.155405
1135.230092	131871.972654	35.160423
1136.591433	132110.421923	35.165440
1137.547706	132363.859526	35.170458
1138.759041	132621.440172	35.175476
1140.080825	132865.922819	35.180493
1141.135877	133131.671535	35.185511
1142.195329	133378.001458	35.190528
1143.185763	133641.001625	35.195546
1143.953160	133900.960351	35.200564
1145.469503	134166.349962	35.205581
1146.087953	134431.129374	35.210599
1147.523676	134696.663440	35.215616
1148.266094	134969.780918	35.220634
1149.650224	135236.760449	35.225652
1150.879321	135509.345765	35.230669
1151.775992	135783.953236	35.235687
1152.841558	136047.886069	35.240704
1153.976423	136326.629682	35.245722
1155.455907	136600.336456	35.250740
1156.732378	136864.494623	35.255757
1157.790409	137138.136001	35.260775
1158.894329	137396.862761	35.265792
1160.039278	137668.757315	35.270810
1161.322582	137926.964174	35.275828
1162.944062	138201.966678	35.280845
1164.117729	138474.002566	35.285863
1165.476411	138715.378882	35.290880
1166.676668	138961.372747	35.295898
1167.852981	139212.583316	35.300916
1168.748398	139466.783614	35.305933
1169.440194	139709.266135	35.310951
1170.959613	139964.952060	35.315968
1171.885562	140225.200922	35.320986
1172.890367	140483.625653	35.326004
1174.060703	140726.949400	35.331021
1174.968899	141002.003858	35.336039
1176.534318	141241.969452	35.341056
1177.465678	141512.307462	35.346074
1178.506327	141782.097028	35.351092
1179.668524	142055.735981	35.356109
1180.573929	142339.576066	35.361127
1182.210140	142596.771406	35.366144
1183.706551	142868.814716	35.371162
1184.882903	143144.843847	35.376180
1186.142473	143404.022079	35.381197
1187.246930	143676.821177	35.386215
1188.594622	143946.995456	35.391232
1189.564981	144220.695902	35.396250
1190.835825	144486.550302	35.401268
1192.031781	144760.357223	35.406285
1193.344542	145038.953037	35.411303
1194.629669	145306.992402	35.416320
1195.790640	145576.271678	35.421338
1196.589019	145864.862810	35.426356
1197.933116	146143.271953	35.431373
1198.933258	146426.647728	35.436391
1200.065384	146706.034685	35.441408
1201.131154	147000.918935	35.446426
1202.106298	147291.445408	35.451444
1203.361658	147570.095917	35.456461
1204.980632	147875.815023	35.461479
1206.123494	148171.621933	35.466496
1207.442842	148453.616744	35.471514
1208.335323	148750.585734	35.476532
1209.541422	149041.468630	35.481549
1210.511167	149344.529876	35.486567
1211.971486	149646.498062	35.491584
1213.210564	149940.959131	35.496602
1214.273156	150250.138220	35.501620
1215.571507	150554.347389	35.506637
1216.847717	150856.216386	35.511655
1218.451348	151143.892277	35.516672
1220.035833	151449.520112	35.521690
1221.217825	151741.341491	35.526708
1222.602988	152025.293349	35.531725
1224.102125	152330.092701	35.536743
1224.916988	152622.095692	35.541760
1226.513591	152898.307700	35.546778
1227.396219	153199.081005	35.551796
1228.995602	153477.871576	35.556813
1230.051593	153769.209438	35.561831
1230.861935	154070.128413	35.566848
1232.252967	154355.618886	35.571866
1233.117606	154660.008974	35.576884
1234.646629	154963.885917	35.581901
1235.650649	155276.033327	35.586919
1237.062081	155567.161288	35.591936
1238.418789	155866.190263	35.596954
1239.024225	156183.700238	35.601972
1240.749509	156474.871995	35.606989
1241.911460	156777.973869	35.612007
1243.280112	157093.766975	35.617024
1244.685972	157380.279387	35.622042
1245.614134	157690.264127	35.627060
1247.148204	157982.848622	35.632077
1247.930282	158270.079337	35.637095
1249.270929	158556.852054	35.642112
1250.496904	158846.779084	35.647130
1251.414289	159156.244244	35.652148
1252.674961	159438.824867	35.657165
1253.647395	159745.532686	35.662183
1254.843913	160057.495868	35.667200
1256.035606	160352.361539	35.672218
1257.185418	160660.239498	35.677236
1258.160945	160971.916347	35.682253
1258.930323	161305.411943	35.687271
1260.111104	161610.881563	35.692288
1261.774691	161937.916891	35.697306
1263.294507	162263.583021	35.702324
1264.401927	162586.211547	35.707341
1265.620506	162911.501143	35.712359
1266.607603	163245.801107	35.717376
1268.299193	163567.490796	35.722394
1269.271545	163905.921733	35.727412
1270.541740	164240.982191	35.732429
1271.716141	164580.019550	35.737447
1273.041906	164912.158080	35.742464
1274.757366	165254.854304	35.747482
1276.141983	165585.377061	35.752500
1277.599622	165925.456826	35.757517
1278.821891	166245.582195	35.762535
1279.839728	166573.762416	35.767552
1281.511411	166927.949048	35.772570
1282.739005	167275.258802	35.777588
1284.129867	167596.444806	35.782605
1285.482287	167943.751961	35.787623
1287.031830	168279.064199	35.792640
1288.356021	168608.795195	35.797658
1289.569970	168948.748443	35.802676
1291.184477	169273.056518	35.807693
1292.021153	169616.452319	35.812711
1293.366226	169960.908840	35.817728
1294.799187	170292.372714	35.822746
1295.649844	170637.969206	35.827764
1297.063399	170987.662845	35.832781
1298.643857	171323.551128	35.837799
1299.678398	171667.006000	35.842816
1301.347276	172006.564618	35.847834
1302.536883	172350.671556	35.852852
1304.255508	172688.729636	35.857869
1305.446452	173026.953416	35.862887
1306.653072	173373.831506	35.867904
1308.115952	173710.974810	35.872922
1309.073244	174051.109990	35.877940
1310.575000	174394.774437	35.882957
1311.897123	174747.163793	35.887975
1313.097198	175097.418569	35.892992
1314.575782	175440.815239	35.898010
1315.810911	175800.650605	35.903028
1317.375802	176127.781506	35.908045
1318.415535	176485.103447	35.913063
1319.738698	176823.015221	35.918080
1321.773125	177151.331932	35.923098
1322.898543	177514.967321	35.928116
1324.407700	177846.243534	35.933133
1325.838937	178191.913813	35.938151
1326.940257	178534.239733	35.943168
1328.499983	178869.550252	35.948186
1329.724594	179211.035556	35.953204
1330.974859	179552.696636	35.958221
1332.092692	179893.823472	35.963239
1332.979075	180235.765000	35.968256
1334.731703	180563.960404	35.973274
1335.483995	180907.324670	35.978292
1337.176689	181233.287837	35.983309
1338.260669	181563.567255	35.988327
1339.382140	181908.324168	35.993344
1340.683360	182241.453152	35.998362
1342.239911	182572.892152	36.003380
1343.301928	182921.079789	36.008397
1344.757143	183259.749063	36.013415
1346.015485	183593.490278	36.018432
1347.169033	183936.414869	36.023450
1348.322281	184285.358003	36.028468
1349.695221	184629.583572	36.033485
1351.793267	184981.193088	36.038503
1353.000927	185338.765162	36.043520
1354.062245	185681.513056	36.048538
1355.301385	186041.508912	36.053556
1356.685210	186397.408789	36.058573
1357.964005	186754.965724	36.063591
1359.332253	187115.696216	36.068608
1361.023254	187481.694290	36.073626
1361.801786	187846.537941	36.078644
1363.429031	188215.635845	36.083661
1364.713645	188589.641659	36.088679
1365.858803	188968.407694	36.093696
1367.268518	189324.728156	36.098714
1368.634816	189715.013952	36.103732
1370.053909	190090.860722	36.108749
1371.797323	190461.794621	36.113767
1372.846554	190850.172850	36.118784
1374.355258	191231.229475	36.123802
1375.499645	191616.080803	36.128820
1376.912576	192007.567530	36.133837
1378.184117	192387.312467	36.138855
1379.833152	192771.542144	36.143872
1381.096143	193161.791738	36.148890
1382.353156	193563.330377	36.153908
1384.043024	193946.481748	36.158925
1385.398289	194334.895612	36.163943
1386.830137	194737.568342	36.168960
1388.333756	195123.436411	36.173978
1389.275283	195522.767520	36.178996
1391.006126	195920.967998	36.184013
1392.807697	196298.808912	36.189031
1394.034305	196692.628763	36.194048
1395.510153	197073.371783	36.199066
1397.215334	197476.194663	36.204084
1398.324329	197869.546032	36.209101
1399.827717	198243.054972	36.214119
1400.992845	198644.882411	36.219136
1402.991963	199041.483683	36.224154
1404.228775	199432.538107	36.229172
1405.358238	199822.355652	36.234189
1406.910322	200218.352132	36.239207
1408.107897	200611.451267	36.244224
1409.478861	201011.126041	36.249242
1410.856088	201422.444522	36.254260
1411.559157	201827.731726	36.259277
1413.119197	202220.996106	36.264295
1414.269840	202628.029688	36.269312
1415.990663	203033.701884	36.274330
1417.305856	203447.226336	36.279348
1418.609158	203873.400992	36.284365
1420.599490	204271.201940	36.289383
1421.815849	204682.248569	36.294400
1423.781494	205082.737061	36.299418
1425.133248	205495.441904	36.304436
1426.569917	205902.535669	36.309453
1428.035911	206288.105323	36.314471
1429.001131	206685.352065	36.319488
1430.546522	207068.627135	36.324506
1432.175327	207458.429452	36.329524
1433.270313	207858.517785	36.334541
1434.878411	208244.391338	36.339559
1435.897678	208647.391241	36.344576
1437.132510	209039.158445	36.349594
1438.411195	209450.855534	36.354612
1439.889413	209860.439413	36.359629
1441.166034	210270.338000	36.364647
1442.250785	210680.829029	36.369664
1443.780414	211098.359489	36.374682
1445.368131	211526.612202	36.379700
1446.736656	211940.199065	36.384717
1448.219069	212350.150244	36.389735
1449.695982	212789.335302	36.394752
1450.851761	213204.245974	36.399770
1452.616098	213635.311927	36.404788
1453.843977	214075.916065	36.409805
1455.380766	214511.366715	36.414823
1456.793175	214943.462263	36.419840
1458.650957	215388.540424	36.424858
1460.457903	215811.482957	36.429876
1462.133077	216240.925478	36.434893
1463.798539	216666.892186	36.439911
1464.826776	217094.159685	36.444928
1466.621212	217521.861442	36.449946
1467.849922	217960.249299	36.454964
1468.951402	218409.733579	36.459981
1470.771395	218844.218241	36.464999
1471.961035	219300.066961	36.470016
1473.541914	219811.957624	36.475034
1474.722273	220263.926397	36.480052
1475.880013	220706.655933	36.485069
1477.498801	221158.632537	36.490087
1479.347283	221621.443799	36.495104
1480.387070	222083.958784	36.500122
1482.269481	222531.453064	36.505140
1483.660130	222988.783537	36.510157
1485.329301	223447.873310	36.515175
1486.548930	223910.925252	36.520192
1488.288415	224364.622635	36.525210
1490.185998	224833.154354	36.530228
1491.052867	225279.506611	36.535245
1493.051181	225748.431846	36.540263
1494.293055	226208.797124	36.545280
1495.938087	226679.562345	36.550298
1496.938982	227155.337869	36.555316
1498.847644	227609.045344	36.560333
1500.403553	228068.629296	36.565351
1501.803922	228546.325467	36.570368
1503.332813	229012.114943	36.575386
1505.094242	229477.207325	36.580404
1506.161625	229948.715180	36.585421
1507.995070	230406.636061	36.590439
1509.376536	230877.993765	36.595456
1510.848579	231359.193589	36.600474
1512.523693	231804.495766	36.605492
1513.916586	232284.670401	36.610509
1515.674275	232751.603392	36.615527
1517.092975	233227.458748	36.620544
1518.381959	233696.173942	36.625562
1520.319960	234164.935901	36.630580
1521.527312	234629.755665	36.635597
1523.404156	235107.141568	36.640615
1524.793028	235583.110744	36.645632
1526.286806	236045.296436	36.650650
1527.695983	236509.605704	36.655668
1528.871855	236964.784786	36.660685
1530.972638	237418.008941	36.665703
1531.961016	237869.944528	36.670720
1533.420597	238325.232742	36.675738
1535.056524	238791.136354	36.680756
1536.446280	239247.733863	36.685773
1537.679821	239695.696185	36.690791
1538.998745	240183.450377	36.695808
1540.604454	240655.764797	36.700826
1542.356294	241126.354260	36.705844
1543.666425	241608.651866	36.710861
1545.653151	242070.263115	36.715879
1546.954288	242549.719256	36.720896
1548.531031	243045.896485	36.725914
1550.319826	243504.952305	36.730932
1551.849337	244003.222354	36.735949
1553.667622	244468.854379	36.740967
1555.336052	244940.583201	36.745984
1557.194967	245425.490794	36.751002
1558.738011	245891.196199	36.756020
1560.568620	246375.551307	36.761037
1562.126576	246844.507381	36.766055
1563.495268	247315.476847	36.771072
1565.105626	247800.200880	36.776090
1566.787081	248289.029184	36.781108
1567.866887	248774.401090	36.786125
1569.710330	249276.210374	36.791143
1570.865574	249757.100289	36.796160
1572.295486	250247.090573	36.801178
1573.870073	250745.770831	36.806196
1575.350820	251247.947396	36.811213
1576.650970	251751.576916	36.816231
1578.354634	252255.978717	36.821248
1579.902586	252776.867954	36.826266
1581.518449	253284.790916	36.831284
1582.687914	253790.019061	36.836301
1584.608627	254303.862377	36.841319
1586.411816	254828.826700	36.846336
1588.158328	255349.736259	36.851354
1589.276400	255857.870428	36.856372
1590.736596	256381.977905	36.861389
1592.684222	256898.130239	36.866407
1594.533388	257419.379725	36.871424
1596.071782	257949.978311	36.876442
1597.657859	258464.844584	36.881460
1599.177186	259007.335404	36.886477
1601.273516	259517.214916	36.891495
1602.527184	260049.994907	36.896512
1604.065770	260575.386379	36.901530
1605.980491	261089.690765	36.906548
1607.608492	261614.610213	36.911565
1609.491852	262140.757634	36.916583
1611.404727	262660.269830	36.921600
1612.739391	263189.301922	36.926618
1614.657618	263691.284680	36.931636
1616.590761	264206.626917	36.936653
1618.105608	264720.742379	36.941671
1619.803303	265235.767335	36.946688
1620.833493	265750.444876	36.951706
1622.838263	266268.949597	36.956724
1624.251709	266785.392248	36.961741
1625.545024	267306.223671	36.966759
1626.969573	267829.370096	36.971776
1628.473124	268360.784432	36.976794
1630.785720	268876.213219	36.981812
1631.844996	269415.574738	36.986829
1633.574042	269949.719121	36.991847
1635.018162	270462.012473	36.996864
1636.568241	270971.849033	37.001882
1638.165124	271489.526731	37.006900
1639.354172	272008.820592	37.011917
1640.641018	272533.330566	37.016935
1642.571589	273054.685198	37.021952
1643.789435	273592.922448	37.026970
1645.992846	274114.357377	37.031988
1647.329405	274638.474709	37.037005
1648.816243	275161.728025	37.042023
1650.695543	275696.016565	37.047040
1652.103799	276238.002546	37.052058
1653.977729	276784.889475	37.057076
1655.537690	277321.589841	37.062093
1657.456185	277860.744723	37.067111
1659.370398	278407.113358	37.072128
1660.877881	278947.984710	37.077146
1662.735391	279483.792771	37.082164
1664.214870	280036.300296	37.087181
1665.911268	280589.710468	37.092199
1667.431481	281135.502214	37.097216
1668.881382	281699.720484	37.102234
1670.731855	282251.043089	37.107252
1672.309474	282823.746618	37.112269
1673.778363	283373.706377	37.117287
1675.668184	283938.835997	37.122304
1677.312770	284501.616517	37.127322
1679.192471	285067.353778	37.132340
1681.005548	285634.675013	37.137357
1682.813933	286201.791850	37.142375
1684.628924	286761.336035	37.147392
1686.331523	287332.682885	37.152410
1688.358467	287893.559682	37.157428
1690.123375	288456.992312	37.162445
1691.489998	289038.116668	37.167463
1693.055036	289603.254300	37.172480
1694.392977	290183.692914	37.177498
1696.201556	290759.149156	37.182516
1698.097797	291330.448237	37.187533
1699.949354	291914.376191	37.192551
1701.948180	292490.301592	37.197568
1703.564646	293066.643098	37.202586
1705.758086	293645.680781	37.207604
1707.530233	294221.483290	37.212621
1708.868462	294790.369752	37.217639
1710.839613	295372.255283	37.222656
1712.436914	295948.840336	37.227674
1713.825142	296519.157982	37.232692
1715.704567	297091.855467	37.237709
1717.165398	297683.769991	37.242727
1719.091100	298263.895745	37.247744
1720.727814	298845.844001	37.252762
1722.448710	299427.775211	37.257780
1724.170320	300019.481524	37.262797
1726.076541	300602.264585	37.267815
1727.856088	301192.964078	37.272832
1729.407952	301779.532394	37.277850
1731.259754	302364.574691	37.282868
1732.909161	302964.936350	37.287885
1734.467312	303546.007152	37.292903
1736.406336	304137.881693	37.297920
1738.078538	304744.171401	37.302938
1739.875987	305327.553673	37.307956
1741.468985	305928.261294	37.312973
1742.928212	306524.796520	37.317991
1744.399468	307121.351171	37.323008
1746.210220	307734.531240	37.328026
1748.054919	308318.241709	37.333044
1749.798016	308912.656729	37.338061
1751.341114	309508.421163	37.343079
1753.143565	310088.266238	37.348096
1754.922007	310678.650368	37.353114
1756.558973	311272.634323	37.358132
1758.716591	311836.460115	37.363149
1760.291510	312420.338537	37.368167
1762.308754	313008.913900	37.373184
1763.805463	313591.247440	37.378202
1765.724854	314170.484924	37.383220
1767.666917	314767.414064	37.388237
1769.266910	315353.018391	37.393255
1771.385496	315931.396910	37.398272
1773.117302	316524.105940	37.403290
1774.834230	317112.064054	37.408308
1776.649613	317705.232158	37.413325
1778.275797	318305.104927	37.418343
1780.376664	318890.318851	37.423360
1781.890031	319496.446733	37.428378
1783.725061	320096.726807	37.433396
1785.675063	320690.710819	37.438413
1786.807622	321311.308264	37.443431
1788.326897	321917.921564	37.448448
1790.653938	322535.542941	37.453466
1792.454902	323157.841135	37.458484
1794.139095	323771.494354	37.463501
1795.616717	324402.213008	37.468519
1797.714892	325015.684525	37.473536
1799.113734	325652.142067	37.478554
1800.925351	326292.638250	37.483572
1803.283971	326919.403342	37.488589
1804.521269	327558.533972	37.493607
1806.709952	328189.477995	37.498624
1808.355162	328830.279819	37.503642
1810.169088	329477.241788	37.508660
1811.718953	330107.509344	37.513677
1813.911682	330759.040863	37.518695
1815.844554	331400.173583	37.523712
1817.952073	332059.067017	37.528730
1819.381623	332699.405102	37.533748
1821.090602	333342.279330	37.538765
1822.351657	334002.203752	37.543783
1824.881641	334661.504854	37.548800
1826.663611	335327.014117	37.553818
1827.935454	335976.657209	37.558836
1830.132940	336643.630372	37.563853
1831.825029	337326.925082	37.568871
1833.747510	337986.082889	37.573888
1835.796842	338656.736082	37.578906
1837.295116	339327.166978	37.583924
1839.388621	339988.124412	37.588941
1841.339292	340656.813493	37.593959
1843.511731	341318.857620	37.598976
1845.498735	341995.264955	37.603994
1847.174941	342660.850757	37.609012
1848.973234	343304.223557	37.614029
1850.973986	343981.591548	37.619047
1853.201822	344643.760008	37.624064
1855.231699	345305.292194	37.629082
1857.154463	345966.426883	37.634100
1859.013639	346626.750756	37.639117
1860.904981	347286.095700	37.644135
1862.762549	347937.366254	37.649152
1864.523361	348600.039013	37.654170
1866.589275	349253.312529	37.659188
1868.728298	349908.721903	37.664205
1870.497760	350574.714806	37.669223
1872.319390	351220.513939	37.674240
1873.856654	351867.264315	37.679258
1875.842414	352515.961534	37.684276
1877.566027	353133.149206	37.689293
1879.127348	353777.558525	37.694311
1881.080980	354420.726361	37.699328
1883.056037	355047.894494	37.704346
1884.675347	355682.445666	37.709364
1886.572750	356310.775486	37.714381
1888.419006	356968.437443	37.719399
1890.140665	357605.353702	37.724416
1892.112443	358264.776325	37.729434
1893.647172	358929.030822	37.734452
1895.112133	359581.386294	37.739469
1896.808943	360243.512374	37.744487
1898.926620	360927.124621	37.749504
1901.325281	361596.927583	37.754522
1903.284380	362263.848877	37.759540
1905.145443	362928.948560	37.764557
1906.905340	363618.713875	37.769575
1908.665171	364289.008428	37.774592
1910.664818	364988.071789	37.779610
1911.773528	365674.255272	37.784628
1913.896454	366367.489400	37.789645
1915.361628	367080.632087	37.794663
1917.302988	367781.633312	37.799680
1919.379090	368509.158863	37.804698
1920.999496	369233.904504	37.809716
1923.172799	369934.979740	37.814733
1924.852496	370662.655784	37.819751
1927.261548	371383.957389	37.824768
1929.067585	372112.370355	37.829786
1930.969138	372858.964572	37.834804
1933.134299	373585.995277	37.839821
1934.851477	374336.191090	37.844839
1936.511776	375071.239085	37.849856
1938.825495	375805.124288	37.854874
1940.311152	376555.235468	37.859892
1942.492232	377307.954937	37.864909
1944.271505	378040.791097	37.869927
1946.460939	378787.821799	37.874944
1948.322850	379550.105988	37.879962
1949.875594	380307.884981	37.884980
1952.286119	381062.234410	37.889997
1954.137819	381842.067609	37.895015
1955.998216	382590.768098	37.900032
1958.322948	383355.983763	37.905050
1960.271629	384118.251805	37.910068
1962.561147	384878.823272	37.915085
1964.643254	385649.477149	37.920103
1966.849399	386393.774690	37.925120
1969.218655	387155.446148	37.930138
1971.320063	387898.560002	37.935156
1973.738516	388640.387389	37.940173
1975.925328	389388.548284	37.945191
1978.185226	390116.930811	37.950208
1980.300049	390847.373793	37.955226
1982.056243	391581.965567	37.960244
1984.228588	392311.578902	37.965261
1986.278974	393049.712345	37.970279
1988.379422	393777.604463	37.975296
1990.415281	394511.776115	37.980314
1992.249289	395243.986260	37.985332
1994.111806	395967.277378	37.990349
1995.940885	396707.284841	37.995367
1997.769597	397446.437662	38.000384
1999.785379	398183.817832	38.005402
2001.565994	398918.101105	38.010420
2003.798517	399635.134120	38.015437
2006.130743	400369.594211	38.020455
2007.657547	401088.329848	38.025472
2009.911261	401793.040676	38.030490
2011.266542	402506.320923	38.035508
2013.589983	403219.499768	38.040525
2015.781874	403938.586579	38.045543
2017.706061	404642.876081	38.050560
2019.846417	405347.289732	38.055578
2021.563177	406067.338204	38.060596
2023.675284	406786.390798	38.065613
2025.499421	407522.700962	38.070631
2027.526727	408247.835704	38.075648
2029.356124	408981.192508	38.080666
2031.169963	409722.335195	38.085684
2032.946555	410455.027807	38.090701
2034.864527	411202.015712	38.095719
2036.710419	411963.611478	38.100736
2038.424340	412716.924036	38.105754
2040.309019	413478.875627	38.110772
2042.231944	414251.412328	38.115789
2044.142474	415041.886920	38.120807
2045.875921	415826.034859	38.125824
2048.322286	416604.722918	38.130842
2050.051648	417417.849240	38.135860
2052.307108	418192.316920	38.140877
2054.122966	419002.339986	38.145895
2056.212623	419815.711125	38.150912
2058.575956	420621.971197	38.155930
2060.412798	421441.865570	38.160948
2062.425826	422246.308428	38.165965
2064.554282	423065.975225	38.170983
2066.579600	423890.189830	38.176000
2069.028028	424712.737519	38.181018
2071.064018	425528.894907	38.186036
2073.516593	426342.627280	38.191053
2075.719877	427166.348654	38.196071
2077.659104	427980.566830	38.201088
2080.478694	428793.397339	38.206106
2082.862325	429602.728321	38.211124
2085.897038	430394.913853	38.216141
2088.490486	431197.524148	38.221159
2090.679129	431987.518117	38.226176
2092.977612	432768.608700	38.231194
2094.629796	433566.130428	38.236212
2096.813926	434350.123306	38.241229
2098.978256	435148.822716	38.246247
2100.777223	435956.766925	38.251264
2102.796828	436733.519120	38.256282
2104.615650	437551.223279	38.261300
2106.387749	438345.473481	38.266317
2108.412027	439143.247634	38.271335
2110.397132	439973.843864	38.276352
2112.737506	440778.643803	38.281370
2114.873515	441599.439154	38.286388
2116.686958	442400.371411	38.291405
2118.956578	443221.489939	38.296423
2121.043315	444029.351740	38.301440
2123.223810	444837.674488	38.306458
2125.005467	445681.145228	38.311476
2127.400609	446504.802165	38.316493
2129.580197	447320.571515	38.321511
2131.480329	448155.680804	38.326528
2133.918977	448961.126857	38.331546
2136.124487	449790.810889	38.336564
2138.115395	450602.490959	38.341581
2140.245685	451428.835922	38.346599
2142.466197	452258.269657	38.351616
2144.883357	453079.950826	38.356634
2146.578735	453907.079764	38.361652
2148.403973	454709.475421	38.366669
2150.669248	455511.969913	38.371687
2152.828293	456313.995784	38.376704
2154.932280	457108.010145	38.381722
2157.063304	457924.642236	38.386740
2158.840845	458717.434682	38.391757
2161.004682	459529.800615	38.396775
2163.071700	460349.329328	38.401792
2165.220506	461168.255262	38.406810
2167.319651	461991.756549	38.411828
2169.300334	462819.641623	38.416845
2171.223518	463658.066838	38.421863
2173.329505	464487.530184	38.426880
2175.981632	465333.801573	38.431898
2177.754933	466178.159857	38.436916
2179.978489	467020.840850	38.441933
2181.909706	467879.857914	38.446951
2183.488173	468742.685560	38.451968
2186.116175	469601.511692	38.456986
2187.778575	470478.650534	38.462004
2190.109731	471379.691407	38.467021
2192.125033	472254.417101	38.472039
2194.428567	473139.716009	38.477056
2196.443031	474028.760025	38.482074
2198.679698	474934.650000	38.487092
2200.790079	475834.758168	38.492109
2203.166945	476729.020406	38.497127
2205.394438	477654.178537	38.502144
2207.802938	478566.784649	38.507162
2210.301541	479475.542798	38.512180
2212.176370	480383.247873	38.517197
2214.385331	481301.812163	38.522215
2216.479934	482230.701773	38.527232
2219.068560	483145.727041	38.532250
2220.998721	484086.011919	38.537268
2222.770098	485043.996950	38.542285
2225.159309	485971.888392	38.547303
2227.192664	486936.141354	38.552320
2229.975410	487879.721750	38.557338
2231.951254	488821.264735	38.562356
2234.112120	489779.385189	38.567373
2236.771581	490725.862559	38.572391
2238.831748	491679.807225	38.577408
2241.086325	492641.137351	38.582426
2243.530721	493598.951096	38.587444
2245.756413	494541.910973	38.592461
2247.986250	495500.815184	38.597479
2250.009509	496469.337640	38.602496
2252.598469	497427.973665	38.607514
2254.850371	498391.252971	38.612532
2256.978454	499356.667270	38.617549
2259.690801	500319.457965	38.622567
2261.634963	501292.964073	38.627584
2264.293984	502244.907992	38.632602
2266.186641	503224.262093	38.637620
2268.671932	504185.606063	38.642637
2270.562625	505169.182898	38.647655
2272.544502	506147.794091	38.652672
2275.279722	507107.766068	38.657690
2277.405431	508089.162071	38.662708
2279.716784	509070.921951	38.667725
2282.112070	510036.323212	38.672743
2284.387289	511016.105240	38.677760
2286.901164	512001.131789	38.682778
2289.207082	512978.872960	38.687796
2291.190957	513952.121004	38.692813
2293.940063	514931.735519	38.697831
2296.073699	515898.085126	38.702848
2299.098337	516835.451791	38.707866
2301.211314	517773.215029	38.712884
2303.601529	518709.414867	38.717901
2306.158400	519628.449342	38.722919
2308.357710	520557.766760	38.727936
2310.679877	521495.824780	38.732954
2313.193988	522422.912095	38.737972
2314.956867	523349.412270	38.742989
2317.452612	524292.811700	38.748007
2319.519536	525248.261598	38.753024
2322.201821	526177.963679	38.758042
2324.250802	527123.023319	38.763060
2326.128527	528069.008638	38.768077
2328.690477	529026.705627	38.773095
2331.021100	529987.350157	38.778112
2333.117864	530946.511022	38.783130
2335.396721	531907.392260	38.788148
2337.751708	532882.143604	38.793165
2340.120440	533844.393990	38.798183
2342.429954	534820.534306	38.803200
2344.857670	535799.408538	38.808218
2347.217572	536788.847740	38.813236
2349.155655	537795.299361	38.818253
2351.522668	538770.862565	38.823271
2353.660189	539788.615763	38.828288
2356.061717	540790.202258	38.833306
2358.252224	541809.060809	38.838324
2360.088388	542823.578194	38.843341
2362.394667	543847.956193	38.848359
2364.835370	544877.066630	38.853376
2367.076769	545918.306703	38.858394
2369.594887	546962.039033	38.863412
2371.732433	548008.119664	38.868429
2374.086125	549050.213845	38.873447
2376.449695	550122.095962	38.878464
2378.677703	551178.632330	38.883482
2381.115528	552234.801477	38.888500
2383.553758	553306.623914	38.893517
2385.913324	554384.708711	38.898535
2388.434623	555453.382578	38.903552
2391.052447	556529.696021	38.908570
2393.356144	557607.985496	38.913588
2395.244569	558697.060814	38.918605
2397.828660	559783.269678	38.923623
2399.925635	560878.363271	38.928640
2402.160318	561989.771846	38.933658
2405.219195	563070.257867	38.938676
2407.180341	564195.842542	38.943693
2409.709987	565290.950690	38.948711
2412.399674	566399.500562	38.953728
2414.883021	567506.634186	38.958746
2417.858596	568614.395560	38.963764
2420.151956	569709.823034	38.968781
2422.713519	570819.019744	38.973799
2425.448927	571912.830974	38.978816
2427.925938	573012.012312	38.983834
2430.717085	574102.363787	38.988852
2432.741879	575205.896916	38.993869
2435.503266	576296.164681	38.998887
2438.217607	577397.886832	39.003904
2440.550600	578472.430840	39.008922
2443.494890	579562.635356	39.013940
2446.002637	580660.692346	39.018957
2448.320997	581736.913493	39.023975
2450.855514	582823.237272	39.028992
2453.103433	583904.296664	39.034010
2455.715665	584991.268669	39.039028
2458.111981	586076.825794	39.044045
2460.138386	587124.743012	39.049063
2462.434911	588186.863803	39.054080
2465.008994	589240.273370	39.059098
2467.222697	590281.269254	39.064116
2469.181113	591353.242297	39.069133
2471.687536	592410.094236	39.074151
2473.964055	593492.999146	39.079168
2475.964228	594563.123650	39.084186
2478.535963	595650.192724	39.089204
2480.517062	596741.567652	39.094221
2483.027072	597849.736131	39.099239
2485.455046	598957.863573	39.104256
2487.323024	600072.589478	39.109274
2489.960961	601189.185183	39.114292
2492.310134	602327.503653	39.119309
2494.669901	603466.209095	39.124327
2497.006965	604612.816198	39.129344
2499.324617	605753.104652	39.134362
2501.946644	606905.242518	39.139380
2504.200059	608083.550815	39.144397
2506.581421	609250.355785	39.149415
2509.093507	610425.275482	39.154432
2512.258938	611595.862353	39.159450
2515.220740	612786.022233	39.164468
2517.347696	613967.889391	39.169485
2520.254596	615129.295498	39.174503
2523.343313	616317.057246	39.179520
2525.639853	617505.872442	39.184538
2528.111538	618686.080441	39.189556
2530.553350	619881.815798	39.194573
2533.249367	621070.879997	39.199591
2536.185029	622257.525927	39.204608
2538.640227	623451.718743	39.209626
2541.501605	624634.268906	39.214644
2543.968175	625834.743792	39.219661
2546.446898	627025.639741	39.224679
2549.540586	628216.302214	39.229696
2551.686218	629415.130722	39.234714
2554.466455	630606.027966	39.239732
2556.532537	631829.421297	39.244749
2558.869617	633032.254848	39.249767
2561.427750	634243.702483	39.254784
2563.704470	635469.584812	39.259802
2566.387280	636690.863931	39.264820
2568.806542	637913.441136	39.269837
2571.271532	639140.408594	39.274855
2573.742866	640383.946445	39.279872
2576.612251	641628.466420	39.284890
2579.599644	642844.729186	39.289908
2582.016875	644085.733328	39.294925
2584.728364	645321.600493	39.299943
2587.151020	646571.578345	39.304960
2590.118497	647804.807354	39.309978
2592.861222	649040.814776	39.314996
2595.310121	650283.399201	39.320013
2597.854308	651530.848606	39.325031
2600.683790	652769.124352	39.330048
2603.144716	654009.150927	39.335066
2605.941966	655249.764588	39.340084
2608.675057	656501.592597	39.345101
2610.994923	657742.719429	39.350119
2613.650291	658980.347019	39.355136
2615.866490	660224.663824	39.360154
2618.707565	661478.479113	39.365172
2621.669533	662731.814264	39.370189
2624.382264	663980.199656	39.375207
2626.931809	665222.477609	39.380224
2629.706849	666462.268843	39.385242
2632.478391	667652.485277	39.390260
2635.060712	668860.945468	39.395277
2637.223887	670076.635138	39.400295
2639.970094	671279.239179	39.405312
2642.464163	672483.174647	39.410330
2645.154266	673690.206757	39.415348
2648.077627	674906.394202	39.420365
2650.489561	676114.702467	39.425383
2653.314134	677314.037254	39.430400
2655.755078	678528.193047	39.435418
2658.318101	679746.742608	39.440436
2661.408545	680970.759802	39.445453
2664.070460	682188.077115	39.450471
2666.731430	683413.083175	39.455488
2669.568976	684648.179108	39.460506
2672.062782	685870.201946	39.465524
2674.519475	687114.314963	39.470541
2676.834215	688351.031774	39.475559
2679.443214	689618.411466	39.480576
2681.478389	690889.381255	39.485594
2684.136044	692154.262087	39.490612
2686.484765	693436.979959	39.495629
2688.705732	694734.569272	39.500647
2691.297649	696038.804529	39.505664
2693.509065	697366.919168	39.510682
2696.318357	698675.046495	39.515700
2698.539508	700006.581907	39.520717
2701.002517	701351.709041	39.525735
2703.826786	702699.247222	39.530752
2706.439407	704068.223068	39.535770
2709.231234	705423.424858	39.540788
2712.091304	706791.831813	39.545805
2714.344631	708171.665542	39.550823
2717.207488	709555.685511	39.555840
2719.925384	710945.102771	39.560858
2722.678855	712324.533533	39.565876
2725.652963	713718.161764	39.570893
2728.158958	715123.073553	39.575911
2731.158976	716529.106215	39.580928
2733.897891	717943.508638	39.585946
2736.589278	719340.611485	39.590964
2739.638541	720757.407864	39.595981
2742.257044	722172.650029	39.600999
2745.268315	723571.613891	39.606016
2748.032351	724991.494968	39.611034
2750.824479	726414.686872	39.616052
2753.815583	727817.285852	39.621069
2756.610008	729245.819754	39.626087
2759.687988	730668.128403	39.631104
2762.181576	732084.110173	39.636122
2765.208422	733501.831817	39.641140
2767.968466	734932.090157	39.646157
2770.725270	736356.812498	39.651175
2773.830441	737774.215116	39.656192
2776.504188	739201.309631	39.661210
2778.942752	740634.701964	39.666228
2781.726731	742058.602216	39.671245
2784.543342	743491.121076	39.676263
2787.373984	744904.438640	39.681280
2790.390747	746341.388776	39.686298
2793.368668	747767.827282	39.691316
2795.789911	749185.027394	39.696333
2798.329444	750639.013456	39.701351
2801.638919	752066.878510	39.706368
2804.300071	753493.799046	39.711386
2807.303380	754921.138496	39.716404
2810.528165	756353.988216	39.721421
2812.900526	757768.393578	39.726439
2815.670214	759157.117967	39.731456
2818.443817	760549.920288	39.736474
2820.854658	761921.070211	39.741492
2823.899228	763323.259776	39.746509
2826.464082	764719.266222	39.751527
2829.195641	766112.527000	39.756544
2831.873505	767515.471584	39.761562
2834.711937	768924.174120	39.766580
2837.819890	770332.713517	39.771597
2840.473336	771742.928457	39.776615
2842.876139	773155.913725	39.781632
2845.643047	774591.561360	39.786650
2848.451277	776021.224198	39.791668
2851.325980	777458.602481	39.796685
2853.671844	778910.810208	39.801703
2856.616804	780365.869889	39.806720
2858.866720	781832.728438	39.811738
2861.557607	783308.491622	39.816756
2864.356092	784797.721426	39.821773
2866.779431	786285.674662	39.826791
2869.700361	787790.352223	39.831808
2872.070265	789311.866160	39.836826
2874.679002	790838.701944	39.841844
2877.897850	792370.205653	39.846861
2880.194688	793917.111078	39.851879
2883.298328	795465.846535	39.856896
2886.198523	797025.685586	39.861914
2889.302470	798574.860774	39.866932
2892.273364	800138.938794	39.871949
2895.219406	801706.193025	39.876967
2898.241051	803281.349915	39.881984
2901.266659	804857.614509	39.887002
2904.285658	806444.181536	39.892020
2907.327811	808011.551763	39.897037
2910.050222	809603.058953	39.902055
2913.005271	811197.039665	39.907072
2915.605836	812799.206902	39.912090
2918.491963	814393.375502	39.917108
2921.575742	816010.236421	39.922125
2924.391427	817617.133035	39.927143
2927.474870	819220.133838	39.932160
2930.630902	820838.404227	39.937178
2933.303830	822464.850498	39.942196
2936.197407	824101.593218	39.947213
2939.198736	825738.351433	39.952231
2942.412895	827354.871914	39.957248
2945.622359	828986.447012	39.962266
2948.747814	830616.410278	39.967284
2952.395966	832236.427588	39.972301
2955.152762	833852.193242	39.977319
2958.584293	835460.237010	39.982336
2961.526037	837063.870830	39.987354
2964.741339	838679.957549	39.992372
2968.028718	840267.596190	39.997389
2970.661714	841883.650096	40.002407
2973.763249	843489.489103	40.007424
2976.662341	845098.552816	40.012442
2979.399847	846713.941697	40.017460
2982.607446	848320.382615	40.022477
2985.337546	849937.471451	40.027495
2987.910955	851548.242125	40.032512
2990.887620	853171.058913	40.037530
2993.804038	854792.296645	40.042548
2996.974173	856421.027951	40.047565
3000.022095	858044.206205	40.052583
3003.053742	859658.033055	40.057600
3005.954854	861283.774858	40.062618
3009.131015	862891.875497	40.067636
3011.966858	864474.984164	40.072653
3014.886102	866054.758765	40.077671
3018.005849	867628.080611	40.082688
3020.974359	869217.678150	40.087706
3023.789248	870809.592329	40.092724
3026.247093	872373.162796	40.097741
3029.146746	873977.677538	40.102759
3032.036602	875576.342832	40.107776
3034.838005	877188.812608	40.112794
3037.362783	878812.687301	40.117812
3040.318091	880439.041190	40.122829
3043.439787	882071.007130	40.127847
3045.978580	883711.697799	40.132864
3048.904599	885378.236360	40.137882
3051.771125	887042.665799	40.142900
3054.319849	888708.311381	40.147917
3057.028231	890409.935085	40.152935
3060.144337	892098.927882	40.157952
3063.571168	893804.542983	40.162970
3066.354559	895520.074129	40.167988
3069.600351	897249.473734	40.173005
3072.317437	898981.132809	40.178023
3075.122246	900711.092050	40.183040
3078.295176	902460.205168	40.188058
3081.232047	904216.419939	40.193076
3083.814498	905981.094731	40.198093
3086.867927	907754.853295	40.203111
3089.482316	909540.335697	40.208128
3092.719376	911342.930967	40.213146
3095.826927	913153.515506	40.218164
3099.006349	914965.319128	40.223181
3102.223982	916773.060197	40.228199
3105.080910	918593.516186	40.233216
3108.473856	920426.812363	40.238234
3111.819225	922261.417084	40.243252
3115.100891	924068.068363	40.248269
3118.017062	925908.317006	40.253287
3121.067592	927749.159854	40.258304
3124.654818	929588.898263	40.263322
3127.496173	931439.430424	40.268340
3130.657237	933283.423917	40.273357
3134.295386	935135.983839	40.278375
3138.041822	936973.711536	40.283392
3141.320122	938810.109078	40.288410
3144.404354	940660.145526	40.293428
3147.860772	942484.417204	40.298445
3151.404240	944320.172855	40.303463
3154.675948	946146.343203	40.308480
3158.118161	947975.374067	40.313498
3161.278835	949794.636907	40.318516
3165.036695	951597.218951	40.323533
3168.549524	953408.937317	40.328551
3172.207734	955218.654523	40.333568
3175.694696	957065.997545	40.338586
3178.911506	958921.106487	40.343604
3182.313689	960754.960529	40.348621
3185.272694	962591.431556	40.353639
3188.172470	964439.637014	40.358656
3191.195474	966267.304198	40.363674
3193.862510	968105.384532	40.368692
3196.848424	969952.389744	40.373709
3200.167363	971809.381471	40.378727
3203.074960	973653.549241	40.383744
3206.194272	975506.254796	40.388762
3208.799205	977384.667725	40.393780
3211.785086	979245.737580	40.398797
3214.952885	981130.233312	40.403815
3217.951570	982998.553622	40.408832
3221.030690	984840.547910	40.413850
3223.610416	986694.583746	40.418868
3226.571390	988535.111173	40.423885
3229.654919	990382.220309	40.428903
3232.452204	992251.527534	40.433920
3235.858768	994121.091347	40.438938
3238.503436	995999.783941	40.443956
3241.715771	997896.215378	40.448973
3244.927715	999795.993189	40.453991
3247.720421	1001705.782581	40.459008
3250.384708	1003611.261225	40.464026
3253.469863	1005557.640383	40.469044
3256.541513	1007507.035529	40.474061
3259.649744	1009477.366605	40.479079
3262.638661	1011447.513071	40.484096
3265.530665	1013421.635671	40.489114
3268.269849	1015428.399727	40.494132
3271.923855	1017439.523545	40.499149
3274.914493	1019459.421938	40.504167
3277.604354	1021497.020158	40.509184
3281.611217	1023533.370717	40.514202
3284.389133	1025591.606567	40.519220
3287.773583	1027642.222120	40.524237
3290.927546	1029719.359240	40.529255
3294.205802	1031793.386105	40.534272
3298.061953	1033855.061990	40.539290
3301.287767	1035954.475418	40.544308
3304.876524	1038029.699600	40.549325
3308.427185	1040121.122329	40.554343
3311.658506	1042225.397833	40.559360
3315.079986	1044314.780412	40.564378
3318.187270	1046418.641604	40.569396
3321.596650	1048524.734252	40.574413
3324.716577	1050629.303354	40.579431
3327.732168	1052757.518694	40.584448
3330.897145	1054882.774265	40.589466
3334.041041	1057033.932534	40.594484
3337.012725	1059175.345243	40.599501
3340.445338	1061323.147761	40.604519
3343.495339	1063490.909487	40.609536
3347.033718	1065654.473176	40.614554
3350.479392	1067830.915760	40.619572
3353.442217	1070005.423542	40.624589
3356.664853	1072188.322147	40.629607
3359.480873	1074384.116976	40.634624
3363.050218	1076591.259544	40.639642
3366.223058	1078814.231711	40.644660
3369.454456	1081025.571514	40.649677
3373.075825	1083247.331925	40.654695
3376.437245	1085480.753138	40.659712
3379.306086	1087705.979368	40.664730
3382.619840	1089941.206858	40.669748
3386.019490	1092174.258111	40.674765
3389.560389	1094435.383396	40.679783
3392.285113	1096699.610745	40.684800
3395.459507	1098952.993050	40.689818
3398.850008	1101231.234802	40.694836
3402.489493	1103507.044491	40.699853
3405.949233	1105768.778444	40.704871
3409.781595	1108056.636174	40.709888
3413.468294	1110327.365892	40.714906
3416.978213	1112572.336124	40.719924
3420.309130	1114858.807139	40.724941
3423.697140	1117127.755091	40.729959
3426.769913	1119397.408894	40.734976
3430.792272	1121653.597465	40.739994
3434.099500	1123932.968210	40.745012
3437.462847	1126188.595109	40.750016
3440.924445	1128385.485234	40.755021
3444.011413	1130519.746224	40.760026
3447.244111	1132589.656200	40.765031
3450.307893	1134597.810444	40.770036
3453.702217	1136519.604569	40.775040
3456.971721	1138348.467498	40.780045
3459.420804	1140124.554659	40.785050
3462.705098	1141797.848736	40.790055
3465.337910	1143410.887777	40.795060
3467.995975	1144924.938368	40.800064
3471.106504	1146370.341250	40.805069
3473.299451	1147752.399466	40.810074
3475.547865	1149046.564069	40.815079
3478.015034	1150256.281777	40.820084
3479.865624	1151400.778694	40.825088
3482.127337	1152490.529875	40.830093
3483.875894	1153508.117983	40.835098
3485.787473	1154466.815500	40.840103
3487.576341	1155357.997580	40.845108
3489.137139	1156197.702129	40.850112
3491.214060	1156977.319066	40.855117
3492.489742	1157713.641093	40.860122
3494.262215	1158381.226786	40.865127
3495.646776	1159004.640103	40.870132
3497.076270	1159584.203621	40.875136
3498.385802	1160114.287640	40.880141
3499.613092	1160597.925390	40.885146
3500.784513	1161037.677039	40.890151
3502.011230	1161445.347675	40.895156
3502.814627	1161801.274734	40.900160
3503.850405	1162122.746338	40.905165
3504.552076	1162427.719064	40.910170
3505.545138	1162684.065376	40.915175
3506.487400	1162911.404571	40.920180
3507.170076	1163112.042062	40.925184
3507.905377	1163287.252022	40.930189
3508.352890	1163462.125658	40.935194
3509.211407	1163557.296029	40.940199
3509.822186	1163658.834209	40.945204
3510.421153	1163738.363836	40.950208
3511.052458	1163798.995700	40.955213
3511.371287	1163828.319102	40.960218
3511.883521	1163840.702972	40.965223
3512.407461	1163842.222512	40.970228
3513.478099	1163817.865606	40.975232
3513.816859	1163784.939127	40.980237
3514.249848	1163726.682349	40.985242
3514.435745	1163638.144306	40.990247
3514.769054	1163555.248134	40.995252
3515.037436	1163453.941187	41.000256
3515.484152	1163325.491578	41.005261
3515.726559	1163211.525920	41.010266
3516.236474	1163075.974767	41.015271
3516.678520	1162932.684596	41.020276
3516.387382	1162768.065503	41.025280
3517.075537	1162589.486169	41.030285
3517.509890	1162410.092221	41.035290
3517.501007	1162225.096054	41.040295
3517.760302	1162029.277545	41.045300
3517.747754	1161814.503617	41.050304
3518.075657	1161610.909823	41.055309
3517.908301	1161395.482748	41.060314
3518.392873	1161160.282683	41.065319
3518.811620	1160933.872158	41.070324
3518.922525	1160693.325735	41.075328
3518.839247	1160440.796633	41.080333
3518.855747	1160199.676011	41.085338
3519.416358	1159927.450229	41.090343
3519.370432	1159674.594503	41.095348
3519.279900	1159410.484233	41.100352
3519.636202	1159121.990198	41.105357
3519.835055	1158851.564454	41.110362
3519.925784	1158562.421582	41.115367
3519.876288	1158281.606787	41.120372
3519.986775	1157976.921246	41.125376
3520.158899	1157677.314472	41.130381
3520.329625	1157396.510634	41.135386
3520.101392	1157097.977031	41.140391
3520.341698	1156789.607292	41.145396
3519.946183	1156485.769810	41.150400
3520.348424	1156174.121282	41.155405
3520.482043	1155864.485102	41.160410
3520.571062	1155547.837264	41.165415
3520.529926	1155230.151069	41.170420
3520.363322	1154907.924749	41.175424
3520.904495	1154592.848024	41.180429
3520.691490	1154278.444404	41.185434
3520.673720	1153934.842645	41.190439
3520.494654	1153619.069139	41.195444
3520.454386	1153284.040779	41.200448
3520.909594	1152960.835589	41.205453
3520.720808	1152635.255527	41.210458
3520.969326	1152302.010241	41.215463
3520.800641	1151966.256501	41.220468
3520.894978	1151626.177635	41.225472
3521.321503	1151281.003973	41.230477
3520.622807	1150939.307088	41.235482
3520.993555	1150594.571078	41.240487
3520.938154	1150247.799296	41.245492
3520.628342	1149908.338989	41.250496
3521.151584	1149566.446517	41.255501
3520.781604	1149221.647989	41.260506
3520.944028	1148869.350675	41.265511
3520.755136	1148519.077044	41.270516
3520.992085	1148170.320555	41.275520
3521.277016	1147814.616806	41.280525
3521.017880	1147480.486972	41.285530
3521.065339	1147126.386691	41.290535
3521.253559	1146769.680878	41.295540
3520.691966	1146417.528600	41.300544
3521.044912	1146060.179108	41.305549
3521.153164	1145710.143940	41.310554
3521.116158	1145351.862932	41.315559
3520.777680	1145009.722332	41.320564
3520.974935	1144650.122826	41.325568
3521.191917	1144283.859094	41.330573
3520.900674	1143932.634261	41.335578
3520.864563	1143586.085063	41.340583
3520.957184	1143223.750796	41.345588
3521.046345	1142860.443946	41.350592
3520.861975	1142503.985619	41.355597
3520.601678	1142137.936354	41.360602
3520.761431	1141781.182956	41.365607
3520.700830	1141428.236144	41.370612
3520.967639	1141066.294567	41.375616
3520.754163	1140713.704748	41.380621
3520.472572	1140354.081708	41.385626
3520.504644	1140000.075634	41.390631
3520.740278	1139637.282442	41.395636
3520.491580	1139281.471660	41.400640
3520.495274	1138925.975024	41.405645
3520.377947	1138576.548690	41.410650
3520.378988	1138209.045773	41.415655
3520.644510	1137857.230980	41.420660
3520.677188	1137500.020250	41.425664
3520.543601	1137135.977494	41.430669
3520.740419	1136789.799329	41.435674
3520.593401	1136421.247473	41.440679
3520.462740	1136050.483357	41.445684
3520.309072	1135698.879307	41.450688
3520.628384	1135328.370481	41.455693
3520.321509	1134973.704655	41.460698
3520.273174	1134612.323916	41.465703
3520.070991	1134248.854204	41.470708
3520.186553	1133909.340605	41.475712
3519.989375	1133551.046936	41.480717
3520.431999	1133198.799115	41.485722
3520.396046	1132835.015278	41.490727
3520.163904	1132474.089415	41.495732
3519.983060	1132123.108236	41.500736
3520.070699	1131767.023002	41.505741
3520.126553	1131408.068026	41.510746
3519.721710	1131050.400273	41.515751
3519.714777	1130695.969702	41.520756
3520.042237	1130348.114428	41.525760
3520.158414	1129981.828963	41.530765
3519.434481	1129627.445304	41.535770
3519.528831	1129285.072985	41.540775
3519.574812	1128922.434137	41.545780
3519.426716	1128580.722035	41.550784
3519.838906	1128229.766657	41.555789
3519.214242	1127884.284573	41.560794
3519.560886	1127527.968117	41.565799
3519.464423	1127180.641480	41.570804
3519.401689	1126830.623303	41.575808
3519.267558	1126475.932733	41.580813
3519.371502	1126144.867230	41.585818
3519.318902	1125781.460030	41.590823
3519.130657	1125439.743373	41.595828
3519.062340	1125098.841425	41.600832
3519.121927	1124746.668141	41.605837
3519.222940	1124411.213462	41.610842
3519.097361	1124064.830602	41.615847
3518.743450	1123719.319442	41.620852
3518.761238	1123372.582522	41.625856
3518.903119	1123039.319249	41.630861
3518.672555	1122699.908962	41.635866
3518.857811	1122350.317486	41.640871
3518.779264	1122009.219883	41.645876
3518.569488	1121668.407751	41.650880
3518.755655	1121321.033862	41.655885
3518.656888	1120989.967607	41.660890
3518.814694	1120651.220217	41.665895
3518.490796	1120307.673674	41.670900
3518.263819	1119979.518270	41.675904
3518.336138	1119645.673827	41.680909
3518.372052	1119308.766430	41.685914
3518.550270	1118971.147563	41.690919
3518.524441	1118628.682452	41.695924
3518.202608	1118299.677490	41.700928
3518.290763	1117960.485355	41.705933
3518.226478	1117633.112002	41.710938
3517.760944	1117295.493460	41.715943
3518.215200	1116962.562209	41.720948
3518.231457	1116642.357470	41.725952
3518.013982	1116301.776391	41.730957
3517.734771	1115971.001079	41.735962
3517.522262	1115642.196055	41.740967
3517.806593	1115317.483317	41.745972
3517.677495	1114989.863759	41.750976
3518.025486	1114657.664796	41.755981
3517.464411	1114338.561515	41.760986
3517.847072	1114010.416460	41.765991
3517.796641	1113678.413161	41.770996
3517.654931	1113364.999459	41.776000
3517.780169	1113026.537807	41.781005
3517.890131	1112703.698215	41.786010
3517.630027	1112373.746884	41.791015
3517.841039	1112056.765114	41.796020
3517.125012	1111727.135268	41.801024
3517.280140	1111404.877847	41.806029
3517.279781	1111091.212688	41.811034
3517.346947	1110770.744307	41.816039
3517.482935	1110441.181409	41.821044
3516.985942	1110126.396771	41.826048
3517.014672	1109809.216962	41.831053
3517.003805	1109497.082648	41.836058
3517.240217	1109175.632415	41.841063
3517.046765	1108856.237992	41.846068
3516.784923	1108536.454077	41.851072
3516.954346	1108215.434707	41.856077
3516.581193	1107915.485934	41.861082
3516.820467	1107607.687183	41.866087
3516.850231	1107291.886093	41.871092
3516.692181	1106973.806055	41.876096
3516.580077	1106652.835293	41.881101
3516.479329	1106363.066777	41.886106
3516.818412	1106043.704098	41.891111
3516.704084	1105740.822274	41.896116
3516.893452	1105432.429889	41.901120
3516.967139	1105113.533270	41.906125
3516.779993	1104808.796415	41.911130
3516.605614	1104483.408582	41.916135
3516.811272	1104169.305707	41.921140
3516.272231	1103855.784818	41.926144
3516.388566	1103545.863559	41.931149
3516.205486	1103247.725097	41.936154
3516.381527	1102931.070940	41.941159
3516.303777	1102627.721443	41.946164
3516.156394	1102326.850787	41.951168
3516.600026	1102022.425830	41.956173
3516.181971	1101717.265524	41.961178
3516.125729	1101407.823219	41.966183
3516.460244	1101109.768040	41.971188
3516.132039	1100808.460181	41.976192
3516.466901	1100496.798428	41.981197
3516.405176	1100192.066709	41.986202
3516.092842	1099881.431960	41.991207
3515.956288	1099578.876724	41.996212
3515.900537	1099279.159507	42.001216
3515.873086	1098974.831503	42.006221
3515.925356	1098663.206105	42.011226
3515.930796	1098359.411743	42.016231
3516.085017	1098074.510675	42.021236
3515.789498	1097775.036404	42.026240
3515.932747	1097474.708148	42.031245
3515.184600	1097181.396558	42.036250
3515.515406	1096879.474011	42.041255
3515.707012	1096597.454156	42.046260
3515.744788	1096307.792001	42.051264
3516.122490	1095996.628932	42.056269
3515.605741	1095706.930269	42.061274
3515.663637	1095402.482770	42.066279
3515.469465	1095101.217203	42.071284
3515.423551	1094806.225880	42.076288
3515.402230	1094521.070855	42.081293
3515.259375	1094231.997193	42.086298
3515.356497	1093933.202508	42.091303
3515.287933	1093645.712279	42.096308
3515.250687	1093355.904499	42.101312
3515.204275	1093075.080308	42.106317
3515.346280	1092784.159517	42.111322
3515.365932	1092494.487742	42.116327
3515.174883	1092197.655112	42.121332
3514.911008	1091914.030270	42.126336
3515.111047	1091626.101427	42.131341
3514.993937	1091353.625187	42.136346
3515.170866	1091059.829377	42.141351
3514.901020	1090774.135042	42.146356
3514.614870	1090494.174211	42.151360
3514.893662	1090200.410843	42.156365
3514.756942	1089922.981705	42.161370
3514.551311	1089639.419843	42.166375
3515.048189	1089369.424635	42.171380
3514.777142	1089091.113035	42.176384
3514.588255	1088813.252602	42.181389
3514.609709	1088521.835625	42.186394
3514.684208	1088236.717359	42.191399
3514.642818	1087957.447579	42.196404
3514.564105	1087688.613317	42.201408
3514.678435	1087409.864623	42.206413
3514.275956	1087133.486516	42.211418
3514.170207	1086858.195418	42.216423
3514.607848	1086574.271696	42.221428
3514.309412	1086307.705301	42.226432
3514.362837	1086029.662550	42.231437
3514.377388	1085762.442808	42.236442
3514.387973	1085483.899966	42.241447
3514.463081	1085218.464725	42.246452
3514.401716	1084937.413449	42.251456
3514.368700	1084660.177677	42.256461
3513.904258	1084388.080056	42.261466
3514.424189	1084108.328293	42.266471
3514.313141	1083824.063739	42.271476
3513.957778	1083573.768495	42.276480
3513.721640	1083287.387005	42.281485
3513.735514	1083023.484917	42.286490
3513.867874	1082765.496373	42.291495
3513.968062	1082493.786436	42.296500
3513.574336	1082233.269873	42.301504
3513.768685	1081960.175066	42.306509
3513.500412	1081706.134833	42.311514
3513.374386	1081440.644373	42.316519
3513.859457	1081183.290194	42.321524
3513.464747	1080923.286703	42.326528
3513.645382	1080646.770669	42.331533
3513.457809	1080398.988101	42.336538
3513.366552	1080145.901332	42.341543
3513.352440	1079881.563795	42.346548
3513.279027	1079619.430201	42.351552
3513.339400	1079366.186311	42.356557
3513.160064	1079122.278740	42.361562
3513.034005	1078861.748800	42.366567
3513.442854	1078599.198839	42.371572
3513.007101	1078347.428974	42.376576
3513.066223	1078106.220075	42.381581
3513.129351	1077846.186379	42.386586
3512.614726	1077591.610992	42.391591
3512.659558	1077340.003462	42.396596
3512.801174	1077100.368463	42.401600
3513.043655	1076847.553687	42.406605
3512.707838	1076601.351082	42.411610
3512.466114	1076348.304913	42.416615
3512.467191	1076098.567660	42.421620
3512.714796	1075869.711233	42.426624
3513.128125	1075623.917316	42.431629
3512.862907	1075375.727304	42.436634
3512.600491	1075138.665612	42.441639
3513.011539	1074890.438215	42.446644
3512.638431	1074635.989817	42.451648
3513.099497	1074385.234110	42.456653
3512.810555	1074144.868043	42.461658
3512.557569	1073904.965767	42.466663
3512.763776	1073647.590307	42.471668
3512.519852	1073413.908960	42.476672
3512.529881	1073163.363649	42.481677
3512.287531	1072925.338033	42.486682
3512.373348	1072679.657847	42.491687
3512.513405	1072432.900792	42.496692
3512.369920	1072199.439265	42.501696
3512.304690	1071970.375055	42.506701
3512.232228	1071718.912372	42.511706
3512.110225	1071487.242728	42.516711
3512.279844	1071248.019205	42.521716
3512.099523	1071020.664066	42.526720
3512.450579	1070771.106349	42.531725
3512.178967	1070531.635868	42.536730
3512.155141	1070302.302813	42.541735
3512.167685	1070064.303015	42.546740
3512.096205	1069836.207908	42.551744
3511.843124	1069598.423873	42.556749
3511.899068	1069372.499514	42.561754
3511.725671	1069148.718694	42.566759
3511.798487	1068909.985850	42.571764
3511.754912	1068682.126538	42.576768
3511.915457	1068444.224297	42.581773
3511.789285	1068222.801706	42.586778
3511.802309	1067991.923543	42.591783
3511.955283	1067765.820827	42.596788
3511.690178	1067545.932414	42.601792
3511.653535	1067310.513839	42.606797
3511.689239	1067076.996774	42.611802
3511.513761	1066855.719457	42.616807
3511.939512	1066630.005905	42.621812
3511.642656	1066407.864859	42.626816
3511.559459	1066165.479272	42.631821
3511.698170	1065963.929835	42.636826
3511.459896	1065733.478987	42.641831
3511.669106	1065509.486628	42.646836
3511.320908	1065284.037613	42.651840
3511.295605	1065057.275404	42.656845
3510.924880	1064843.068753	42.661850
3511.414802	1064634.581370	42.666855
3511.697626	1064400.428633	42.671860
3511.488206	1064175.969720	42.676864
3511.486145	1063949.639090	42.681869
3511.144288	1063730.284025	42.686874
3511.077420	1063500.769821	42.691879
3511.179362	1063295.086454	42.696884
3511.108410	1063081.242929	42.701888
3510.798971	1062857.901592	42.706893
3510.958869	1062650.740815	42.711898
3510.601481	1062434.320439	42.716903
3511.183210	1062229.962068	42.721908
3511.081305	1062013.964376	42.726912
3510.837299	1061795.478613	42.731917
3510.932115	1061579.335181	42.736922
3510.802207	1061380.261175	42.741927
3511.050440	1061153.389079	42.746932
3510.927884	1060949.387982	42.751936
3510.665424	1060725.181999	42.756941
3510.660898	1060527.115634	42.761946
3510.627182	1060317.684179	42.766951
3511.016287	1060099.411955	42.771956
3511.023227	1059888.224092	42.776960
3511.019525	1059685.312186	42.781965
3510.980469	1059464.677674	42.786970
3510.688833	1059255.248277	42.791975
3510.783984	1059037.945527	42.796980
3510.795759	1058831.532191	42.801985
3510.695380	1058628.597266	42.806989
3510.722205	1058428.812731	42.811994
3510.307934	1058214.547557	42.816999
3510.465383	1058005.863662	42.822004
3510.375505	1057810.892697	42.827009
3510.707521	1057594.746409	42.832013
3510.365160	1057395.466920	42.837018
3510.245284	1057187.086734	42.842023
3510.448706	1056992.134845	42.847028
3510.194583	1056791.277327	42.852033
3510.383786	1056581.570713	42.857037
3510.443039	1056370.913891	42.862042
3510.457378	1056178.277101	42.867047
3510.327272	1055971.009038	42.872052
3510.452209	1055780.845790	42.877057
3510.382163	1055569.890545	42.882061
3510.373724	1055371.543040	42.887066
3510.121794	1055184.698271	42.892071
3510.355343	1054970.585803	42.897076
3509.927110	1054766.695171	42.902081
3510.063817	1054569.162440	42.907085
3510.080350	1054372.220825	42.912090
3510.146007	1054170.829595	42.917095
3510.363189	1053974.322750	42.922100
3509.809716	1053792.107951	42.927105
3510.200266	1053583.411119	42.932109
3510.153689	1053388.565880	42.937114
3509.888393	1053197.124462	42.942119
3510.025743	1052994.039373	42.947124
3509.801268	1052807.784558	42.952129
3509.870032	1052608.553630	42.957133
3509.606634	1052417.181288	42.962138
3510.046312	1052232.147736	42.967143
3510.019305	1052039.373269	42.972148
3509.574000	1051840.102857	42.977153
3509.603262	1051640.554201	42.982157
3509.721464	1051458.633986	42.987162
3509.390978	1051274.081006	42.992167
3509.744845	1051084.007611	42.997172
3509.729457	1050891.287637	43.002177
3509.761222	1050702.990466	43.007181
3509.707922	1050514.411495	43.012186
3509.600697	1050334.613673	43.017191
3509.596516	1050140.611589	43.022196
3509.311035	1049955.235379	43.027201
3509.504559	1049751.732460	43.032205
3509.492138	1049582.314321	43.037210
3509.312523	1049402.980543	43.042215
3509.567347	1049206.008459	43.047220
3509.613279	1049024.695496	43.052225
3509.619715	1048849.269298	43.057229
3509.415574	1048669.819299	43.062234
3509.188453	1048474.830531	43.067239
3509.589131	1048290.347032	43.072244
3509.264119	1048109.933736	43.077249
3509.320500	1047922.599450	43.082253
3509.520481	1047742.666785	43.087258
3509.290801	1047560.386102	43.092263
3509.499695	1047367.602939	43.097268
3509.024591	1047197.801918	43.102273
3509.179847	1047006.173293	43.107277
3509.496860	1046826.481171	43.112282
3509.124194	1046645.352277	43.117287
3509.456418	1046458.309163	43.122292
3509.073588	1046278.521459	43.127297
3509.155153	1046105.023267	43.132301
3508.933100	1045923.942516	43.137306
3508.842660	1045739.648046	43.142311
3508.923020	1045555.222763	43.147316
3508.603688	1045397.603030	43.152321
3508.814349	1045232.553114	43.157325
3508.750924	1045060.301351	43.162330
3508.547494	1044884.687550	43.167335
3509.122603	1044712.223244	43.172340
3508.740579	1044549.857935	43.177345
3508.567447	1044376.733872	43.182349
3508.930088	1044204.095617	43.187354
3508.812855	1044044.376019	43.192359
3508.616097	1043856.366451	43.197364
3508.876534	1043690.779543	43.202369
3508.621944	1043513.875146	43.207373
3508.386457	1043344.979014	43.212378
3508.576963	1043186.922677	43.217383
3508.951033	1043017.240020	43.222388
3508.505945	1042841.214915	43.227393
3508.385059	1042663.488580	43.232397
3508.282652	1042506.813556	43.237402
3508.448351	1042344.486670	43.242407
3508.506147	1042172.994740	43.247412
3508.278901	1042013.524623	43.252417
3508.354413	1041851.488020	43.257421
3508.114267	1041689.981776	43.262426
3508.246555	1041530.535188	43.267431
3508.214034	1041367.052904	43.272436
3508.147800	1041214.103825	43.277441
3508.267279	1041057.061456	43.282445
3508.214995	1040882.648880	43.287450
3508.388149	1040713.605359	43.292455
3508.075989	1040555.266980	43.297460
3508.216669	1040410.572686	43.302465
3507.936912	1040249.900857	43.307469
3508.133768	1040093.011783	43.312474
3507.815681	1039934.173437	43.317479
3507.944948	1039769.167723	43.322484
3508.153315	1039616.419387	43.327489
3507.840157	1039459.596433	43.332493
3507.922295	1039316.623155	43.337498
3507.870241	1039164.098603	43.342503
3508.373339	1038988.568464	43.347508
3507.946059	1038845.086960	43.352513
3507.984320	1038674.746942	43.357517
3507.923838	1038528.780055	43.362522
3507.481965	1038375.041287	43.367527
3508.032669	1038219.587907	43.372532
3508.005240	1038071.283245	43.377537
3507.996613	1037916.396931	43.382541
3507.504609	1037753.270735	43.387546
3507.565699	1037606.872875	43.392551
3507.858621	1037458.112340	43.397556
3507.536745	1037319.408759	43.402561
3507.587193	1037158.399774	43.407565
3507.718871	1037005.108855	43.412570
3507.359573	1036870.461692	43.417575
3507.650951	1036723.712558	43.422580
3507.740127	1036571.383756	43.427585
3507.575373	1036421.220257	43.432589
3507.445661	1036271.917361	43.437594
3507.640076	1036125.265139	43.442599
3507.721389	1035973.404852	43.447604
3507.457389	1035833.010455	43.452609
3507.478283	1035688.986804	43.457613
3507.737491	1035536.698413	43.462618
3507.604470	1035380.311095	43.467623
3507.585298	1035244.020886	43.472628
3507.399752	1035099.532332	43.477633
3507.627223	1034959.034951	43.482637
3507.816938	1034815.251112	43.487642
3507.519441	1034674.929768	43.492647
3507.732265	1034515.752445	43.497652
3507.194805	1034365.594884	43.502657
3507.142047	1034215.450192	43.507661
3507.276999	1034079.106096	43.512666
3507.144653	1033948.511197	43.517671
3507.201762	1033798.337171	43.522676
3507.435150	1033662.934253	43.527681
3507.081223	1033523.754312	43.532685
3506.889874	1033380.867080	43.537690
3506.992862	1033240.637172	43.542695
3507.035916	1033102.929603	43.547700
3507.486549	1032960.119391	43.552705
3507.094550	1032829.250714	43.557709
3507.441652	1032698.450784	43.562714
3507.204458	1032546.549542	43.567719
3507.171649	1032400.514152	43.572724
3506.927462	1032264.768815	43.577729
3506.930485	1032128.205170	43.582733
3506.973947	1032000.342459	43.587738
3506.793113	1031869.319677	43.592743
3507.069834	1031722.538023	43.597748
3507.032826	1031588.097193	43.602753
3506.945128	1031461.792465	43.607757
3507.068346	1031318.703774	43.612762
3506.946050	1031182.040808	43.617767
3506.929260	1031050.971786	43.622772
3506.772074	1030909.951693	43.627777
3506.979926	1030773.998814	43.632781
3506.975612	1030639.723368	43.637786
3506.919608	1030512.811068	43.642791
3507.138815	1030371.424934	43.647796
3506.652462	1030236.057372	43.652801
3506.570975	1030116.692117	43.657805
3506.739704	1029982.469182	43.662810
3506.916072	1029857.924299	43.667815
3506.927506	1029708.615925	43.672820
3506.732610	1029581.898992	43.677825
3506.839186	1029442.444490	43.682829
3506.878567	1029319.459482	43.687834
3506.611167	1029193.714026	43.692839
3506.692384	1029051.155153	43.697844
3506.793361	1028924.761934	43.702849
3506.546938	1028782.928068	43.707853
3506.666362	1028662.917582	43.712858
3506.604113	1028534.024410	43.717863
3506.780254	1028408.188216	43.722868
3506.647900	1028296.249902	43.727873
3506.426550	1028159.916667	43.732877
3506.656414	1028036.387766	43.737882
3506.514599	1027910.011581	43.742887
3506.543794	1027781.860870	43.747892
3506.614133	1027649.244722	43.752897
3506.408192	1027529.457211	43.757901
3506.629495	1027405.818921	43.762906
3506.396115	1027282.155916	43.767911
3506.534320	1027154.941578	43.772916
3506.572687	1027025.318930	43.777921
3506.368906	1026907.164590	43.782925
3506.323471	1026767.183973	43.787930
3506.475265	1026638.018060	43.792935
3506.255502	1026523.152191	43.797940
3506.258291	1026419.970388	43.802945
3506.075318	1026287.944979	43.807949
3506.338391	1026152.354968	43.812954
3506.092759	1026045.622261	43.817959
3506.206841	1025927.491755	43.822964
3506.088623	1025813.757308	43.827969
3505.890912	1025696.545335	43.832973
3506.409794	1025571.945421	43.837978
3506.039984	1025451.946581	43.842983
3505.896714	1025332.683083	43.847988
3505.949927	1025217.842344	43.852993
3506.052030	1025098.242719	43.857997
3506.310606	1024994.314137	43.863002
3505.933889	1024883.801372	43.868007
3505.975147	1024744.240406	43.873012
3505.877712	1024636.293428	43.878017
3505.962866	1024530.931070	43.883021
3505.955308	1024410.074874	43.888026
3505.744085	1024290.121908	43.893031
3506.230633	1024173.637628	43.898036
3505.918265	1024071.239803	43.903041
3505.932906	1023945.523644	43.908045
3506.065267	1023826.182642	43.913050
3505.938082	1023723.747960	43.918055
3506.036716	1023596.653093	43.923060
3505.867241	1023492.573273	43.928065
3505.586230	1023377.652893	43.933069
3505.843566	1023267.100704	43.938074
3505.483169	1023167.505499	43.943079
3505.739682	1023042.504760	43.948084
3505.872495	1022940.788479	43.953089
3505.650558	1022822.356948	43.958093
3505.687186	1022724.142673	43.963098
3505.396031	1022618.709366	43.968103
3505.537144	1022506.707057	43.973108
3505.511690	1022409.370062	43.978113
3505.623860	1022299.695287	43.983117
3505.661699	1022189.836691	43.988122
3505.517274	1022093.580344	43.993127
3505.516297	1021976.161086	43.998132
3505.430948	1021863.310562	44.003137
3505.548560	1021767.296343	44.008141
3505.494117	1021665.490791	44.013146
3505.521186	1021562.797245	44.018151
3505.822154	1021442.698919	44.023156
3505.512852	1021341.220366	44.028161
3505.335747	1021228.760068	44.033165
3505.467070	1021115.567878	44.038170
3505.521787	1021023.624303	44.043175
3505.431822	1020923.653715	44.048180
3505.494849	1020817.158367	44.053185
3505.488682	1020716.103476	44.058189
3505.604697	1020612.698993	44.063194
3505.430204	1020516.226535	44.068199
3505.430324	1020404.011463	44.073204
3505.350825	1020299.954492	44.078209
3505.319455	1020207.332777	44.083213
3505.287970	1020099.190491	44.088218
3505.165794	1020010.751236	44.093223
3505.274887	1019898.217110	44.098228
3505.441027	1019809.436203	44.103233
3505.593622	1019707.172994	44.108237
3505.440807	1019604.667216	44.113242
3505.208559	1019497.613429	44.118247
3505.353234	1019380.212819	44.123252
3505.435218	1019298.616182	44.128257
3505.324890	1019191.245444	44.133261
3505.399538	1019083.163103	44.138266
3505.623239	1018975.830241	44.143271
3505.755974	1018880.443207	44.148276
3505.313645	1018783.694012	44.153281
3505.013966	1018679.740266	44.158285
3505.390759	1018573.247662	44.163290
3505.285178	1018485.169705	44.168295
3505.044349	1018365.288784	44.173300
3505.297495	1018269.580467	44.178305
3505.302710	1018183.323017	44.183309
3505.252184	1018070.681509	44.188314
3504.997910	1017988.830126	44.193319
3504.979820	1017887.532185	44.198324
3504.966141	1017796.226208	44.203329
3505.025809	1017697.434916	44.208333
3505.129202	1017598.440611	44.213338
3505.060928	1017510.729369	44.218343
3505.377692	1017416.063461	44.223348
3505.177408	1017301.781502	44.228353
3504.906063	1017209.829130	44.233357
3505.224277	1017115.254960	44.238362
3504.591673	1017035.101759	44.243367
3504.905193	1016935.867074	44.248372
3504.993877	1016846.081573	44.253377
3504.679493	1016755.584607	44.258381
3504.860767	1016663.160528	44.263386
3504.480200	1016573.545010	44.268391
3505.064433	1016468.919458	44.273396
3505.092716	1016385.639363	44.278401
3504.659206	1016295.154597	44.283405
3504.789815	1016197.101716	44.288410
3504.660749	1016117.143654	44.293415
3504.784346	1016034.619163	44.298420
3505.146603	1015937.397180	44.303425
3504.806236	1015845.725037	44.308429
3504.999617	1015751.633824	44.313434
3504.688961	1015667.913570	44.318439
3504.458990	1015579.325163	44.323444
3504.448064	1015492.349537	44.328449
3504.696798	1015400.378953	44.333453
3504.788012	1015318.528813	44.338458
3504.495693	1015232.857518	44.343463
3504.683671	1015143.028456	44.348468
3504.991987	1015059.197186	44.353473
3504.600593	1014980.431131	44.358477
3505.023720	1014883.180900	44.363482
3504.564566	1014795.588729	44.368487
3504.890846	1014706.118255	44.373492
3504.887441	1014625.729927	44.378497
3504.734920	1014531.286910	44.383501
3504.862395	1014419.999236	44.388506
3504.706957	1014337.495794	44.393511
3504.982358	1014258.415610	44.398516
3504.829738	1014168.044504	44.403521
3504.513398	1014086.729045	44.408525
3504.938361	1013981.792178	44.413530
3504.334305	1013901.880830	44.418535
3504.278938	1013814.886576	44.423540
3504.504457	1013730.952052	44.428545
3504.578652	1013644.807767	44.433549
3504.669577	1013549.337106	44.438554
3504.698668	1013489.028377	44.443559
3504.556654	1013385.533295	44.448564
3504.835834	1013312.168694	44.453569
3504.460600	1013226.577586	44.458573
3504.123533	1013152.147040	44.463578
3504.305210	1013075.784874	44.468583
3504.512832	1012986.597956	44.473588
3504.415284	1012906.297677	44.478593
3504.285860	1012835.713483	44.483597
3504.441630	1012747.599635	44.488602
3504.627033	1012672.785330	44.493607
3504.364614	1012587.263034	44.498612
3504.334279	1012500.924210	44.503617
3504.412474	1012420.490929	44.508621
3504.347597	1012332.212667	44.513626
3504.371639	1012257.322291	44.518631
3504.296278	1012172.831314	44.523636
3504.734030	1012093.305452	44.528641
3504.401134	1012021.384700	44.533645
3504.656383	1011926.733658	44.538650
3504.650368	1011845.723224	44.543655
3504.449459	1011759.206845	44.548660
3504.748621	1011680.086531	44.553665
3504.802957	1011590.028484	44.558669
3504.661040	1011494.561324	44.563674
3504.503282	1011425.712684	44.568679
3504.652042	1011332.526358	44.573684
3505.020870	1011256.400137	44.578689
3504.302003	1011175.206024	44.583693
3504.500946	1011086.087586	44.588698
3504.532261	1011012.928161	44.593703
3504.351185	1010921.538082	44.598708
3504.664588	1010830.648004	44.603713
3504.496395	1010745.567974	44.608717
3504.457793	1010649.195063	44.613722
3504.565731	1010593.991676	44.618727
3504.416945	1010502.395160	44.623732
3504.650332	1010412.094472	44.628737
3504.501650	1010333.417660	44.633741
3504.285252	1010258.928963	44.638746
3504.543519	1010174.741714	44.643751
3504.382917	1010090.913698	44.648756
3504.320692	1010012.023824	44.653761
3503.772319	1009942.249697	44.658765
3504.358416	1009862.570763	44.663770
3504.016915	1009787.999271	44.668775
3504.398895	1009704.367657	44.673780
3504.352603	1009625.858448	44.678785
3504.321071	1009553.759354	44.683789
3504.171116	1009480.609890	44.688794
3504.115067	1009394.324850	44.693799
3503.816745	1009318.087981	44.698804
3504.316798	1009255.324007	44.703809
3504.303005	1009168.445462	44.708813
3504.267480	1009088.663618	44.713818
3503.811630	1009021.584002	44.718823
3504.077067	1008950.400136	44.723828
3504.095678	1008868.370963	44.728833
3503.983986	1008794.137217	44.733837
3504.025446	1008710.838527	44.738842
3503.975776	1008646.603272	44.743847
3503.999844	1008574.288110	44.748852
3504.035911	1008498.179461	44.753857
3503.555279	1008435.956676	44.758861
3504.119764	1008353.052536	44.763866
3503.962536	1008292.232855	44.768871
3503.691108	1008214.810252	44.773876
3503.868535	1008153.059156	44.778881
3504.031018	1008093.351078	44.783885
3503.870292	1008006.770438	44.788890
3503.838453	1007945.926369	44.793895
3504.034611	1007862.006440	44.798900
3503.979448	1007794.651810	44.803905
3503.715222	1007726.261523	44.808909
3503.960569	1007650.204171	44.813914
3503.751342	1007583.164017	44.818919
3503.831081	1007515.103359	44.823924
3504.123423	1007455.464355	44.828929
3504.125740	1007374.582692	44.833933
3503.909195	1007303.263004	44.838938
3503.585509	1007244.209306	44.843943
3503.999582	1007175.700625	44.848948
3503.885463	1007100.570029	44.853953
3503.754674	1007023.885659	44.858957
3503.847617	1006954.454986	44.863962
3503.873962	1006885.228872	44.868967
3503.673758	1006828.386594	44.873972
3503.983202	1006751.334343	44.878977
3503.747622	1006697.413309	44.883981
3504.093554	1006607.908210	44.888986
3503.754037	1006546.030221	44.893991
3503.885905	1006478.434617	44.898996
3503.613479	1006411.682636	44.904001
3503.567707	1006342.850671	44.909005
3503.665993	1006270.882687	44.914010
3503.535826	1006214.508853	44.919015
3503.772755	1006150.878611	44.924020
3503.599129	1006072.729846	44.929025
3503.562483	1006021.783914	44.934029
3503.513594	1005954.406283	44.939034
3503.369619	1005894.433706	44.944039
3503.698941	1005823.880564	44.949044
3504.164632	1005756.610303	44.954049
3503.809244	1005699.490485	44.959053
3503.925863	1005624.593964	44.964058
3503.954946	1005545.334828	44.969063
3503.907554	1005475.033868	44.974068
3503.627676	1005409.438217	44.979073
3503.406641	1005357.349686	44.984077
3503.620070	1005293.032914	44.989082
3503.690767	1005229.516925	44.994087
3503.488559	1005163.613872	44.999092
3503.922396	1005095.562976	45.004097
3503.244140	1005041.796281	45.009101
3503.455317	1004968.139785	45.014106
3503.754791	1004903.901669	45.019111
3503.712364	1004847.986019	45.024116
3503.757870	1004775.229612	45.029121
3503.572550	1004714.473241	45.034125
3503.767032	1004653.361879	45.039130
3503.744656	1004589.951291	45.044135
3503.685707	1004531.603684	45.049140
3503.803742	1004453.578995	45.054145
3503.669191	1004394.367045	45.059149
3503.473832	1004332.149236	45.064154
3503.166206	1004269.365628	45.069159
3503.316053	1004195.125556	45.074164
3503.392005	1004136.070765	45.079169
3503.032671	1004092.455793	45.084173
3503.007440	1004031.082079	45.089178
3503.111679	1003978.538166	45.094183
3503.039424	1003921.061896	45.099188
3503.286079	1003869.174424	45.104193
3503.223338	1003822.784840	45.109197
3503.271238	1003751.960365	45.114202
3503.061701	1003685.068500	45.119207
3502.969874	1003639.265864	45.124212
3502.946364	1003595.883578	45.129217
3502.921827	1003542.286752	45.134221
3503.013150	1003475.634695	45.139226
3502.898126	1003433.920016	45.144231
3503.102886	1003384.369759	45.149236
3503.028329	1003331.362867	45.154241
3502.880167	1003295.392346	45.159245
3502.909184	1003235.849460	45.164250
3502.834478	1003190.915936	45.169255
3502.508048	1003136.683985	45.174260
3502.758524	1003088.485622	45.179265
3502.474790	1003051.952154	45.184269
3502.532376	1002995.223388	45.189274
3502.445992	1002953.597735	45.194279
3502.657645	1002909.295838	45.199284
3502.869310	1002875.111901	45.204289
3502.552825	1002831.966589	45.209293
3502.905590	1002774.603242	45.214298
3502.652903	1002740.397678	45.219303
3502.444782	1002690.325582	45.224308
3502.958935	1002634.296355	45.229313
3503.163563	1002587.560710	45.234317
3503.183193	1002539.298394	45.239322
3503.004904	1002494.376394	45.244327
3502.863469	1002452.464225	45.249332
3502.994823	1002387.933325	45.254337
3502.846868	1002353.610870	45.259341
3502.821180	1002297.180720	45.264346
3502.928864	1002253.474621	45.269351
3502.856915	1002194.229303	45.274356
3502.927884	1002149.263507	45.279361
3502.475011	1002117.908955	45.284365
3502.573491	1002051.530849	45.289370
3502.907967	1002020.240687	45.294375
3502.843691	1001975.198477	45.299380
3503.021593	1001926.126407	45.304385
3502.919993	1001866.687927	45.309389
3503.400346	1001817.078554	45.314394
3502.967090	1001777.252943	45.319399
3502.855101	1001728.324214	45.324404
3503.039901	1001669.128420	45.329409
3502.803436	1001632.577987	45.334413
3502.778300	1001577.600257	45.339418
3502.965281	1001526.868899	45.344423
3502.662796	1001476.898910	45.349428
3502.458460	1001439.076833	45.354433
3502.708839	1001391.350614	45.359437
3502.958895	1001339.536703	45.364442
3502.798891	1001311.048965	45.369447
3502.792801	1001262.196080	45.374452
3502.699716	1001216.665979	45.379457
3502.485921	1001177.481231	45.384461
3502.728597	1001129.656756	45.389466
3502.710315	1001084.891844	45.394471
3502.561891	1001033.627375	45.399476
3502.691620	1000999.348286	45.404481
3502.596713	1000951.675232	45.409485
3502.902287	1000905.979646	45.414490
3502.940658	1000861.690264	45.419495
3502.558913	1000811.824777	45.424500
3502.937051	1000772.247748	45.429505
3502.641163	1000728.304359	45.434509
3502.866277	1000663.933014	45.439514
3502.904041	1000627.428245	45.444519
3502.706923	1000582.591485	45.449524
3502.978048	1000535.146628	45.454529
3502.761643	1000495.665591	45.459533
3502.911437	1000443.081334	45.464538
3502.468941	1000409.087585	45.469543
3502.656043	1000359.805757	45.474548
3503.218181	1000316.399190	45.479553
3502.558572	1000271.344131	45.484557
3502.875114	1000226.030600	45.489562
3503.010993	1000173.932820	45.494567
3502.539483	1000125.049438	45.499572
3502.685022	1000084.143174	45.504577
3502.448778	1000051.184034	45.509581
3502.693859	1000000.040068	45.514586
3502.719467	999961.683533	45.519591
3502.520345	999907.788993	45.524596
3503.024607	999864.777873	45.529601
3502.429490	999833.823436	45.534605
3502.587885	999787.169632	45.539610
3502.705759	999737.504415	45.544615
3502.495801	999700.353051	45.549620
3502.906537	999653.559241	45.554625
3502.821105	999621.935615	45.559629
3502.833729	999563.038203	45.564634
3502.642307	999516.439786	45.569639
3502.578180	999481.307297	45.574644
3503.050318	999426.810870	45.579649
3502.544282	999386.104233	45.584653
3502.604300	999336.152973	45.589658
3502.520143	999313.386456	45.594663
3502.367910	999279.338103	45.599668
3502.468718	999221.201437	45.604673
3502.222491	999189.309815	45.609677
3502.701002	999153.599145	45.614682
3502.423978	999112.463397	45.619687
3502.266741	999078.804085	45.624692
3502.876975	999037.716374	45.629697
3502.419989	998995.927918	45.634701
3502.454580	998966.520097	45.639706
3502.461029	998910.440314	45.644711
3502.647861	998874.970650	45.649716
3502.822228	998841.060589	45.654721
3502.633492	998795.624124	45.659725
3502.610263	998742.663135	45.664730
3502.486817	998712.403763	45.669735
3502.696973	998657.943099	45.674740
3502.844285	998612.060357	45.679745
3502.445946	998572.303769	45.684749
3502.437756	998527.614339	45.689754
3502.575137	998507.242245	45.694759
3502.593212	998467.221600	45.699764
3502.508159	998410.178264	45.704769
3501.877670	998390.321692	45.709773
3502.032534	998361.767239	45.714778
3502.564056	998318.642541	45.719783
3502.329890	998280.901628	45.724788
3502.652327	998243.653015	45.729793
3502.663867	998217.458345	45.734797
3502.859020	998156.958308	45.739802
3503.033434	998109.898569	45.744807
3502.499794	998080.287619	45.749812
3502.683524	998022.709244	45.754817
3502.307471	997971.746654	45.759821
3502.348543	997857.322431	45.764826
3502.200086	997703.780387	45.769831
3502.285941	997498.290273	45.774836
3502.536318	997212.225733	45.779841
3502.110047	996878.048168	45.784845
3502.012019	996472.207255	45.789850
3501.907923	996004.288821	45.794855
3501.898687	995495.303255	45.799860
3501.883144	994895.178165	45.804865
3501.758505	994243.267350	45.809869
3501.887971	993513.668400	45.814874
3501.651045	992725.556932	45.819879
3501.662115	991865.745060	45.824884
3501.456179	990929.012096	45.829889
3501.026843	989934.531343	45.834893
3501.346235	988861.923397	45.839898
3501.027327	987708.641276	45.844903
3500.620639	986484.692941	45.849908
3500.529641	985187.819479	45.854913
3500.212791	983824.503374	45.859917
3499.856374	982358.343340	45.864922
3499.774753	980825.639493	45.869927
3499.541709	979224.552632	45.874932
3499.465360	977526.634507	45.879937
3499.287604	975765.958848	45.884941
3498.815570	973907.198827	45.889946
3498.839185	971970.574045	45.894951
3498.245986	969963.626658	45.899956
3498.083310	967864.379436	45.904961
3497.525586	965668.069728	45.909965
3497.043819	963395.278752	45.914970
3496.902646	961052.342010	45.919975
3496.428614	958635.168280	45.924980
3496.346278	956125.007267	45.929985
3495.731876	953561.002731	45.934989
3495.509642	950963.113363	45.939994
3494.783948	948275.907911	45.944999
3494.334795	945501.520237	45.950004
3493.626327	942652.654152	45.955009
3493.177210	939752.126486	45.960013
3492.367913	936747.572752	45.965018
3491.850193	933665.408305	45.970023
3491.542160	930521.181227	45.975028
3491.338081	927277.995509	45.980033
3490.468410	923967.359513	45.985037
3489.794551	920564.382362	45.990042
3489.362416	917097.211616	45.995047
3488.603409	913547.524827	46.000052
3487.871041	909914.735054	46.005057
3487.022831	906202.290612	46.010061
3486.575387	902402.338226	46.015066
3485.721928	898536.884843	46.020071
3484.688200	894595.627719	46.025076
3483.884139	890569.559577	46.030081
3482.998184	886471.262516	46.035085
3482.602206	882306.134629	46.040090
3481.923558	878058.284004	46.045095
3480.943460	873720.575752	46.050100
3480.575918	869289.098868	46.055105
3479.310592	864809.311038	46.060109
3478.486223	860228.786850	46.065114
3477.663156	855572.225855	46.070119
3476.664404	850841.176677	46.075124
3475.781906	846010.893807	46.080129
3474.979887	841125.776818	46.085133
3474.323782	836154.633879	46.090138
3473.186342	831094.479798	46.095143
3472.017439	825966.491282	46.100148
3471.256770	820739.901443	46.105153
3470.023099	815461.730490	46.110157
3469.391835	810072.674547	46.115162
3468.465193	804608.278326	46.120167
3467.115820	799070.106250	46.125172
3465.976186	793448.550919	46.130177
3464.929351	787747.325220	46.135181
3463.836654	781969.421366	46.140186
3463.064543	776100.869130	46.145191
3460.960996	770152.827430	46.150196
3460.445192	764127.551884	46.155201
3459.062039	758054.604143	46.160205
3457.988347	751854.949749	46.165210
3456.939614	745595.796131	46.170215
3455.649155	739254.359961	46.175220
3454.582436	732817.125770	46.180225
3453.148074	726318.935694	46.185229
3451.970500	719723.864547	46.190234
3450.541553	713047.490319	46.195239
3448.432038	706288.043091	46.200244
3447.387124	699458.755527	46.205249
3445.673953	692558.801038	46.210253
3444.204612	685562.667395	46.215258
3443.146520	678517.049251	46.220263
3441.619986	671390.663332	46.225268
3440.181979	664161.779947	46.230273
3438.495654	656874.235335	46.235277
3437.147010	649494.875541	46.240282
3435.637493	642051.705783	46.245287
3433.932758	634535.750107	46.250292
3432.471756	626923.406532	46.255297
3430.713799	619256.337552	46.260301
3429.387525	611506.444067	46.265306
3427.638543	603671.414818	46.270311
3425.760721	595764.972865	46.275316
3424.040079	587782.639608	46.280321
3422.043444	579740.720580	46.285325
3420.304257	571616.555479	46.290330
3418.735820	563413.872558	46.295335
3417.109169	555150.952137	46.300340
3415.147655	546794.046249	46.305345
3413.024973	538385.794320	46.310349
3411.217137	529894.785263	46.315354
3409.410558	521325.281572	46.320359
3407.300370	512699.400987	46.325364
3405.127194	504003.678193	46.330369
3403.143910	495245.821080	46.335373
3401.413776	486413.799548	46.340378
3399.319771	477503.274331	46.345383
3397.128836	468550.241638	46.350388
3394.836120	459506.621182	46.355393
3393.061461	450404.983740	46.360397
3390.171857	441241.605148	46.365402
3388.190943	432015.761933	46.370407
3385.303126	422736.025897	46.375412
3383.458735	413381.340294	46.380417
3380.883016	403973.283393	46.385421
3378.340932	394489.087856	46.390426
3376.038521	384969.073309	46.395431
3373.543675	375405.661790	46.400436
3370.975280	365772.664975	46.405441
3368.064726	356084.871263	46.410445
3365.570668	346334.936553	46.415450
3363.011565	336556.366486	46.420455
3360.060228	326731.152108	46.425460
3357.500681	316841.730729	46.430465
3354.353549	306913.246659	46.435469
3351.504240	296939.056718	46.440474
3348.641714	286923.643193	46.445479
3345.551521	276867.328623	46.450484
3342.312873	266764.866504	46.455489
3339.059514	256631.509185	46.460493
3335.747056	246468.205608	46.465498
3332.504527	236277.103041	46.470503
3328.708335	226017.059647	46.475508
3325.655565	215709.758372	46.480513
3322.060800	205448.185163	46.485517
3318.477055	195154.285931	46.490522
3314.394163	184828.656052	46.495527
3310.066754	174512.838684	46.500532
3306.012038	164185.605462	46.505537
3301.700245	153851.748407	46.510541
3297.679040	143513.679802	46.515546
3293.097647	133179.671115	46.520551
3288.016829	122871.949006	46.525556
3283.054925	112561.955831	46.530561
3277.567368	102274.347081	46.535565
3272.160015	92037.149606	46.540570
3266.188527	81834.257267	46.545575
3259.293318	71670.079564	46.550580
3252.440217	61599.129863	46.555585
3243.582180	51622.861873	46.560589
3232.902815	41796.735679	46.565594
3210.179749	32431.493608	46.570599
3174.714650	23663.532510	46.575604
3127.258368	15680.639107	46.580609
3073.515531	8588.671282	46.585613
3017.341771	2466.253930	46.590618
2855.556924	417.171473	46.595623
2691.247501	419.420135	46.600628
2630.472976	409.634567	46.605633
2654.689356	400.276957	46.610637
2722.893766	387.279762	46.615642
2797.249473	355.385558	46.620647
2851.971317	379.474130	46.625652
2880.725858	381.883184	46.630657
2887.657853	378.475812	46.635661
2880.713796	366.455276	46.640666
2869.494206	358.658140	46.645671
2858.431714	357.910794	46.650676
2850.782850	354.611756	46.655681
2845.643039	359.829532	46.660685
2843.642366	354.427400	46.665690
2842.900977	351.865317	46.670695
2841.755256	357.362781	46.675700
2840.122088	343.085258	46.680705
2837.692734	345.221729	46.685709
2834.726347	349.673251	46.690714
2831.733739	348.453986	46.695719
2828.244136	350.641436	46.700724
2825.797672	342.718689	46.705729
2822.691018	333.303173	46.710733
2819.084474	339.024991	46.715738
2816.288373	334.481711	46.720743
2813.053108	341.888174	46.725748
2809.803980	335.312938	46.730753
2806.672557	342.223695	46.735757
2803.976464	342.287342	46.740762
2800.494308	335.899008	46.745767
2797.172360	345.816607	46.750772
2793.628602	341.389294	46.755777
2790.565458	332.748485	46.760781
2787.464938	333.571591	46.765786
2784.382201	332.362766	46.770791
2780.484797	341.724590	46.775796
2777.409133	330.619995	46.780801
2773.839289	334.289613	46.785805
2770.841193	328.863123	46.790810
2767.600047	321.014305	46.795815
2764.343225	329.371942	46.800820
2760.810028	324.957116	46.805825
2757.285934	327.950395	46.810829
2753.896772	325.593212	46.815834
2750.956250	323.001055	46.820839
2747.542174	313.116543	46.825844
2743.983856	305.195334	46.830849
2740.577591	321.156010	46.835853
2736.771512	327.388653	46.840858
2733.340185	313.837709	46.845863
2730.194047	326.266177	46.850868
2727.195057	309.108262	46.855873
2723.699437	299.755663	46.860877
2720.446230	314.311276	46.865882
2716.524120	315.684624	46.870887
2712.909956	313.088120	46.875892
2709.567795	306.265558	46.880897
2706.797489	304.814551	46.885901
2703.146937	313.003889	46.890906
2699.948846	308.998428	46.895911
2695.883876	303.537642	46.900916
2692.991365	313.601892	46.905921
2689.900384	315.017086	46.910925
2686.112482	298.314356	46.915930
2682.856814	293.549660	46.920935
2679.106097	302.655571	46.925940
2675.324231	313.800156	46.930945
2671.849822	297.271083	46.935949
2668.104045	302.624925	46.940954
2664.800501	303.699092	46.945959
2661.496446	310.825106	46.950964
2658.331357	298.429803	46.955969
2654.933380	297.968647	46.960973
2651.121114	296.198935	46.965978
2647.585058	294.578532	46.970983
2644.439963	303.662441	46.975988
2641.173065	288.277450	46.980993
2638.197634	293.834295	46.985997
2634.058655	303.227404	46.991002
2631.095883	298.855338	46.996007
2626.924806	300.179804	47.001012
2623.293512	293.662462	47.006017
2620.079505	300.064191	47.011021
2616.420771	292.015477	47.016026
2613.452162	290.577274	47.021031
2610.236862	306.893320	47.026036
2606.339909	295.956322	47.031041
2602.983246	296.254748	47.036045
2599.637177	296.487302	47.041050
2596.123013	283.008531	47.046055
2592.456970	295.569305	47.051060
2589.068690	291.438395	47.056065
2585.682532	284.913016	47.061069
2581.633618	286.785629	47.066074
2578.908715	281.058179	47.071079
2574.928459	287.851556	47.076084
2571.763241	279.699103	47.081089
2568.635290	280.509254	47.086093
2564.582781	287.487595	47.091098
2561.503145	280.049718	47.096103
2557.391653	289.311052	47.101108
2554.389826	287.386643	47.106113
2551.085575	287.164417	47.111117
2547.284993	286.322581	47.116122
2543.945521	281.770470	47.121127
2540.395151	281.664996	47.126132
2536.911161	283.874130	47.131137
2533.122545	280.003520	47.136141
2529.657723	278.501953	47.141146
2526.309255	270.783549	47.146151
2523.107596	282.353208	47.151156
2519.393915	276.003520	47.156161
2516.251573	264.907736	47.161165
2512.768237	281.304974	47.166170
2509.115160	282.160800	47.171175
2505.320351	276.354879	47.176180
2501.616712	277.445070	47.181185
2498.435876	282.165177	47.186189
2495.241123	275.308467	47.191194
2491.849004	283.023038	47.196199
2488.120850	278.946055	47.201204
2484.659050	274.434076	47.206209
2481.175546	268.136826	47.211213
2477.200457	276.033857	47.216218
2473.952862	270.448095	47.221223
2470.638644	277.561433	47.226228
2467.132523	276.264020	47.231233
2463.806676	273.708697	47.236237
2460.642315	272.171428	47.241242
2457.254868	266.532179	47.246247
2453.430865	277.284308	47.251252
2449.814530	275.167282	47.256257
2446.272884	268.076962	47.261261
2442.443139	270.849759	47.266266
2438.998744	274.936560	47.271271
2435.448012	266.040543	47.276276
2432.295052	263.423183	47.281281
2428.894814	269.103713	47.286285
2425.044027	272.855116	47.291290
2422.168445	256.683782	47.296295
2418.597593	280.292021	47.301300
2414.809627	272.377311	47.306305
2411.363544	268.603792	47.311309
2407.712840	268.745095	47.316314
2404.544795	267.569050	47.321319
2401.003214	267.094990	47.326324
2397.264241	271.104304	47.331329
2393.817171	273.524950	47.336333
2390.104147	272.292279	47.341338
2386.617191	257.746140	47.346343
2383.176268	273.259449	47.351348
2380.106269	264.845444	47.356353
2376.514259	261.773292	47.361357
2372.710704	268.553001	47.366362
2369.434560	263.831995	47.371367
2365.951798	264.812028	47.376372
2362.730013	268.615504	47.381377
2359.111591	259.575312	47.386381
2355.139937	267.769574	47.391386
2352.149786	255.442210	47.396391
2348.492231	260.571487	47.401396
2344.841178	259.600224	47.406401
2341.714201	251.165256	47.411405
2337.807620	261.410327	47.416410
2334.343249	257.274342	47.421415
2330.983811	259.597885	47.426420
2327.695085	257.630323	47.431425
2324.167723	255.207553	47.436429
2320.240249	250.533222	47.441434
2316.606122	248.632793	47.446439
2313.176431	256.103320	47.451444
2310.129743	263.893968	47.456449
2307.061707	252.692030	47.461453
2302.842512	257.321126	47.466458
2299.662459	258.145404	47.471463
2296.278178	252.981346	47.476468
2292.449868	254.543750	47.481473
2289.117529	258.230425	47.486477
2285.848626	256.563279	47.491482
2281.965514	259.473699	47.496487
2278.332780	264.113226	47.501492
2275.069715	262.707055	47.506497
2271.690234	251.589159	47.511501
2268.069868	258.836125	47.516506
2264.785121	251.941207	47.521511
2261.077549	259.091175	47.526516
2257.036847	262.684555	47.531521
2253.756004	263.198330	47.536525
2250.107744	265.800501	47.541530
2247.231932	248.208158	47.546535
2243.946277	255.707045	47.551540
2240.340994	256.611744	47.556545
2237.031714	253.064368	47.561549
2233.183697	256.208463	47.566554
2229.528151	243.424828	47.571559
2225.592154	251.992988	47.576564
2222.292860	257.341145	47.581569
2219.213280	250.836932	47.586573
2215.380914	245.145313	47.591578
2211.971557	248.070757	47.596583
2208.567050	248.274547	47.601588
2204.977518	253.696429	47.606593
2202.074734	249.784476	47.611597
2198.046781	256.943608	47.616602
2194.458453	243.611425	47.621607
2190.838380	249.595069	47.626612
2187.336699	243.553052	47.631617
2184.258612	241.404310	47.636621
2180.614513	255.528543	47.641626
2177.779692	243.151292	47.646631
2174.019528	245.129501	47.651636
2169.772064	245.743161	47.656641
2166.835013	240.291419	47.661645
2163.197964	249.262241	47.666650
2159.501289	248.284291	47.671655
2156.088411	248.014453	47.676660
2152.305314	242.563557	47.681665
2149.201612	246.324253	47.686669
2145.770172	247.161450	47.691674
2142.292154	244.284408	47.696679
2138.423136	243.652473	47.701684
2134.685460	243.576115	47.706689
2131.471451	248.724466	47.711693
2127.961176	246.631844	47.716698
2124.854399	237.464689	47.721703
2121.275923	240.944104	47.726708
2117.693634	235.987526	47.731713
2114.129196	249.059386	47.736717
2110.632375	251.745457	47.741722
2107.173689	245.116387	47.746727
2103.558464	241.017346	47.751732
2099.884996	248.842778	47.756737
2096.524217	247.429329	47.761741
2092.807390	240.813253	47.766746
2089.406142	237.385897	47.771751
2086.080676	248.948462	47.776756
2082.608890	232.815115	47.781761
2079.487760	239.265524	47.786765
2075.826902	246.776341	47.791770
2072.390808	233.784359	47.796775
2068.869937	238.233165	47.801780
2064.719488	244.104078	47.806785
2061.406309	233.106987	47.811789
2057.947586	239.725166	47.816794
2054.887643	240.449033	47.821799
2051.369606	239.447097	47.826804
2047.828336	243.388336	47.831809
2044.175042	227.403349	47.836813
2040.122837	239.193341	47.841818
2036.645126	244.700140	47.846823
2033.394536	237.617692	47.851828
2030.125033	232.031832	47.856833
2026.629744	233.250861	47.861837
2022.898505	240.279926	47.866842
2019.608504	236.970399	47.871847
2016.112744	236.856661	47.876852
2012.983898	242.094103	47.881857
2009.479166	236.321921	47.886861
2005.512222	236.677189	47.891866
2002.017397	233.488475	47.896871
1998.891790	227.428923	47.901876
1994.887050	234.308270	47.906881
1991.904984	235.527987	47.911885
1988.040261	240.842537	47.916890
1984.692927	228.831612	47.921895
1981.189293	229.480028	47.926900
1977.613641	234.966206	47.931905
1974.235072	234.761629	47.936909
1970.773976	234.459975	47.941914
1967.200832	235.641560	47.946919
1963.245983	238.153854	47.951924
1959.994406	230.112966	47.956929
1956.790459	232.058712	47.961933
1952.973827	236.084980	47.966938
1949.450123	236.212857	47.971943
1945.989524	223.456253	47.976948
1942.023539	227.224415	47.981953
1938.948150	227.537704	47.986957
1935.755983	232.952741	47.991962
1932.671912	230.702596	47.996967
1928.955335	233.063819	48.001972
1925.167128	231.472650	48.006977
1921.577647	229.289119	48.011981
1917.639076	231.924043	48.016986
1914.605445	228.320700	48.021991
1911.041915	227.120148	48.026996
1907.704770	234.566575	48.032001
1904.380711	221.063532	48.037005
1900.612924	231.995010	48.042010
1897.024314	235.979147	48.047015
1893.792953	217.817361	48.052020
1890.007166	224.739556	48.057025
1886.663410	227.730576	48.062029
1882.827856	224.468801	48.067034
1879.654151	226.522256	48.072039
1876.464055	232.308317	48.077044
1872.436006	233.499294	48.082049
1869.144215	227.967312	48.087053
1865.458752	229.164615	48.092058
1862.039198	224.576154	48.097063
1858.306624	221.362319	48.102068
1854.740845	224.792994	48.107073
1851.538053	227.852226	48.112077
1848.308675	223.827984	48.117082
1844.779455	220.657854	48.122087
1840.934736	215.582146	48.127092
1837.526622	228.068912	48.132097
1834.001491	223.337371	48.137101
1830.255155	229.883421	48.142106
1826.907720	218.900217	48.147111
1823.617503	224.895983	48.152116
1819.950216	229.547916	48.157121
1817.167066	226.403874	48.162125
1812.921414	229.098100	48.167130
1809.398466	228.011362	48.172135
1806.177022	220.625601	48.177140
1802.313162	227.595050	48.182145
1799.187378	217.398381	48.187149
1795.379186	224.652051	48.192154
1792.138738	217.546263	48.197159
1788.540246	223.200946	48.202164
1784.844944	230.534653	48.207169
1781.542831	223.185002	48.212173
1777.903158	217.796695	48.217178
1774.378002	220.445858	48.222183
1771.085293	219.221410	48.227188
1767.623855	220.426588	48.232193
1764.120005	211.855037	48.237197
1760.768829	228.087089	48.242202
1757.031525	221.953473	48.247207
1753.291956	222.501230	48.252212
1749.537872	232.987838	48.257217
1746.495844	225.841339	48.262221
1743.058667	223.423226	48.267226
1739.873760	217.523449	48.272231
1736.016948	223.067269	48.277236
1732.218962	223.651214	48.282241
1728.836067	204.181906	48.287245
1725.445532	223.684493	48.292250
1721.974035	218.401950	48.297255
1718.769579	222.973613	48.302260
1714.766369	223.812716	48.307265
1712.024755	219.420870	48.312269
1708.017184	217.939713	48.317274
1704.537429	222.318848	48.322279
1701.039925	219.727014	48.327284
1697.676005	226.553048	48.332289
1693.891002	219.511615	48.337293
1690.275059	220.135589	48.342298
1687.104797	220.934538	48.347303
1683.707265	220.935373	48.352308
1679.684954	223.483214	48.357313
1676.411944	215.589172	48.362317
1672.804266	224.164062	48.367322
1669.347220	216.986052	48.372327
1666.075604	211.194445	48.377332
1662.483265	213.564104	48.382337
1659.280160	219.208747	48.387341
1655.492020	225.588532	48.392346
1651.936456	219.686329	48.397351
1648.297474	216.558193	48.402356
1644.831621	227.986503	48.407361
1641.442154	209.312908	48.412365
1637.847893	217.702589	48.417370
1634.458121	216.206443	48.422375
1630.865287	220.000299	48.427380
1627.486401	211.666093	48.432385
1623.733924	212.078520	48.437389
1619.860740	217.084165	48.442394
1616.937021	217.725947	48.447399
1613.598077	205.123322	48.452404
1609.624464	219.264806	48.457409
1606.647415	211.546704	48.462413
1602.571388	209.507760	48.467418
1599.643649	218.617163	48.472423
1595.945352	210.234365	48.477428
1592.359425	211.607857	48.482433
1588.965877	214.834622	48.487437
1585.404015	218.685837	48.492442
1581.761921	212.103221	48.497447
1578.311548	209.387458	48.502452
1574.896347	223.237622	48.507457
1571.560542	207.856152	48.512461
1567.726849	212.304311	48.517466
1564.160176	209.619389	48.522471
1560.719142	203.399614	48.527476
1556.978378	219.676871	48.532481
1554.064778	219.759604	48.537485
1550.404534	220.843395	48.542490
1546.769445	206.583822	48.547495
1543.635028	215.006075	48.552500
1539.686961	214.839553	48.557505
1536.329795	211.497453	48.562509
1532.647618	216.682742	48.567514
1529.265262	217.560566	48.572519
1526.471844	215.571828	48.577524
1522.466069	212.826898	48.582529
1519.048964	213.914185	48.587533
1515.060680	215.351158	48.592538
1511.966542	212.506197	48.597543
1508.348683	205.715213	48.602548
1504.056957	216.832164	48.607553
1501.183400	218.191625	48.612557
1497.678036	211.028891	48.617562
1494.210767	212.127527	48.622567
1491.279274	221.339201	48.627572
1487.202045	210.791358	48.632577
1483.936630	190.973534	48.637581
1480.531826	213.736436	48.642586
1476.642487	210.736235	48.647591
1473.379283	201.761893	48.652596
1469.604640	206.036091	48.657601
1466.855466	213.642442	48.662605
1463.049766	201.830424	48.667610
1459.176522	202.012284	48.672615
1455.570555	204.348084	48.677620
1452.136792	204.296014	48.682625
1448.804583	197.833310	48.687629
1444.965563	208.674212	48.692634
1442.074055	201.862342	48.697639
1438.450350	205.320327	48.702644
1434.826719	205.229359	48.707649
1431.202824	200.894960	48.712653
1427.747870	204.358839	48.717658
1424.434693	206.444481	48.722663
1420.891720	206.201203	48.727668
1417.099084	211.476399	48.732673
1413.505051	200.706801	48.737677
1410.189229	208.724756	48.742682
1406.745862	211.436161	48.747687
1403.209544	205.382452	48.752692
1399.601507	202.917444	48.757697
1396.316909	195.957481	48.762701
1392.397733	209.204330	48.767706
1389.063596	206.888275	48.772711
1385.769406	201.862365	48.777716
1381.946133	213.424830	48.782721
1379.225596	199.150968	48.787725
1375.557301	200.823671	48.792730
1371.626847	205.780287	48.797735
1368.246963	200.779974	48.802740
1364.359417	214.830990	48.807745
1361.529152	202.528333	48.812749
1357.616610	194.541541	48.817754
1354.001159	203.603321	48.822759
1351.013034	200.284659	48.827764
1347.145385	201.867356	48.832769
1343.709882	197.062501	48.837773
1339.838099	208.005045	48.842778
1336.361798	202.001649	48.847783
1333.298979	210.699837	48.852788
1329.727114	207.856274	48.857793
1326.279164	198.494113	48.862797
1322.640285	197.131881	48.867802
1319.161059	198.560999	48.872807
1315.776867	203.633667	48.877812
1312.091274	203.473179	48.882817
1308.406401	196.457691	48.887821
1305.073315	205.492122	48.892826
1301.711437	197.448507	48.897831
1298.356307	191.997734	48.902836
1294.694266	207.180222	48.907841
1291.146848	200.181812	48.912845
1287.597570	207.299347	48.917850
1283.863095	206.068933	48.922855
1280.474287	196.917829	48.927860
1276.672207	197.541563	48.932865
1273.391793	190.056132	48.937869
1270.107613	187.160876	48.942874
1267.007813	190.799521	48.947879
1263.601460	193.659474	48.952884
1259.801399	190.074144	48.957889
1256.356613	193.249037	48.962893
1252.837384	192.022870	48.967898
1249.116609	198.904528	48.972903
1245.567753	191.183341	48.977908
1241.837246	198.386449	48.982913
1238.335198	196.917128	48.987917
1234.474475	196.384754	48.992922
1231.172907	193.867573	48.997927
1228.282587	195.932730	49.002932
1224.944599	200.396110	49.007937
1221.598043	195.800587	49.012941
1217.728517	204.160899	49.017946
1213.940882	204.872552	49.022951
1210.580288	197.309625	49.027956
1206.792192	196.131317	49.032961
1203.497894	188.604513	49.037965
1200.209814	202.730656	49.042970
1196.541920	195.846309	49.047975
1192.991864	197.960209	49.052980
1189.474239	206.570151	49.057985
1186.061999	191.447019	49.062989
1182.342353	194.047667	49.067994
1179.069213	203.185507	49.072999
1176.055633	196.938006	49.078004
1171.605672	192.735982	49.083009
1168.243986	186.908316	49.088013
1164.651572	196.681818	49.093018
1161.778428	193.256955	49.098023
1158.653174	186.079233	49.103028
1154.438302	195.965362	49.108033
1151.025775	192.993784	49.113037
1147.400455	190.473366	49.118042
1143.884187	197.338083	49.123047
1140.531752	197.029459	49.128052
1136.600162	196.044567	49.133057
1133.401002	191.942601	49.138061
1129.719777	194.059541	49.143066
1126.447185	196.502755	49.148071
1123.432581	190.178501	49.153076
1119.616685	199.970371	49.158081
1116.013012	195.139539	49.163085
1112.121679	192.697882	49.168090
1109.135577	184.820143	49.173095
1105.804474	188.490431	49.178100
1102.074815	192.061568	49.183105
1098.635647	185.931036	49.188109
1095.092119	194.210353	49.193114
1090.818310	197.057031	49.198119
1087.706919	188.212743	49.203124
1084.420654	186.160047	49.208129
1080.889241	176.510732	49.213133
1077.802599	194.691034	49.218138
1073.899337	196.548595	49.223143
1070.451195	190.926449	49.228148
1066.467208	196.722440	49.233153
1063.337197	190.117654	49.238157
1060.368978	192.168313	49.243162
1056.668572	187.595390	49.248167
1053.204292	193.422096	49.253172
1049.148195	195.599192	49.258177
1045.965699	181.011322	49.263181
1042.443940	183.140946	49.268186
1038.481600	184.826656	49.273191
1035.309303	191.499274	49.278196
1031.839627	190.613887	49.283201
1028.576296	188.179781	49.288205
1025.114748	202.192557	49.293210
1021.309211	186.933415	49.298215
1018.070105	188.206920	49.303220
1014.136826	204.086205	49.308225
1010.650713	195.367357	49.313229
1007.353092	192.418812	49.318234
1003.498114	191.470876	49.323239
1000.318407	193.112727	49.328244
996.768397	181.778344	49.333249
993.638050	180.921401	49.338253
990.159337	198.739781	49.343258
986.255897	191.160954	49.348263
983.224422	178.953305	49.353268
979.534566	195.314092	49.358273
975.951214	176.133171	49.363277
972.300631	184.577997	49.368282
968.821131	180.108746	49.373287
965.259920	184.210921	49.378292
961.640642	188.154578	49.383297
958.389082	189.292148	49.388301
954.613051	186.391942	49.393306
951.143860	192.787461	49.398311
947.960107	188.398427	49.403316
944.668987	185.564664	49.408321
940.607464	190.154737	49.413325
937.177682	193.106119	49.418330
933.838122	191.565440	49.423335
930.303450	190.995682	49.428340
927.014299	200.863842	49.433345
923.216084	183.171520	49.438349
919.986703	181.663957	49.443354
916.133957	190.258704	49.448359
912.739715	191.822960	49.453364
909.026146	185.828510	49.458369
905.534411	191.337607	49.463373
902.176823	192.549635	49.468378
898.504241	194.527644	49.473383
895.962781	184.751479	49.478388
892.156016	193.721527	49.483393
888.263336	179.704740	49.488397
884.899318	187.139514	49.493402
881.106137	196.614906	49.498407
878.017097	182.059261	49.503412
873.944019	182.536871	49.508417
870.600752	175.169488	49.513421
867.081637	184.032062	49.518426
863.563159	178.379529	49.523431
860.363011	179.053659	49.528436
856.679085	193.432914	49.533441
853.187347	190.310710	49.538445
849.568672	183.318913	49.543450
846.156915	194.003392	49.548455
843.052700	180.719275	49.553460
839.508797	194.238033	49.558465
836.037841	191.948310	49.563469
832.455911	193.423930	49.568474
828.371726	183.652658	49.573479
825.221555	187.952704	49.578484
821.541732	187.266982	49.583489
818.181709	183.346437	49.588493
814.712714	190.446084	49.593498
811.314437	180.762027	49.598503
807.801445	176.997467	49.603508
804.083569	182.645764	49.608513
801.051359	180.553924	49.613517
797.158176	181.755400	49.618522
793.400344	187.581074	49.623527
790.132231	181.714690	49.628532
786.625172	182.288496	49.633537
783.256105	181.519219	49.638541
779.871208	182.031322	49.643546
775.803977	180.778902	49.648551
772.892850	176.929769	49.653556
769.174173	183.142324	49.658561
765.295189	181.400868	49.663565
761.953681	183.168991	49.668570
758.380795	182.858983	49.673575
755.182880	178.711334	49.678580
751.476190	178.567463	49.683585
748.179893	186.564690	49.688589
744.670721	178.603153	49.693594
740.808020	181.267117	49.698599
737.631842	175.010695	49.703604
734.159075	179.637031	49.708609
730.871456	184.769573	49.713613
727.299013	174.153338	49.718618
723.464781	169.898194	49.723623
720.465428	177.919394	49.728628
716.668881	179.233800	49.733633
712.889573	171.086737	49.738637
709.513997	171.088179	49.743642
705.670407	173.736378	49.748647
702.640913	166.893915	49.753652
699.248700	180.364875	49.758657
695.631121	181.814883	49.763661
692.083723	178.959651	49.768666
688.283440	179.322276	49.773671
685.083973	175.130133	49.778676
681.672108	180.693916	49.783681
677.922879	170.164527	49.788685
674.618813	176.619315	49.793690
670.972116	174.495446	49.798695
667.771403	182.299636	49.803700
663.940218	175.081522	49.808705
660.528907	160.531411	49.813709
657.316747	173.774447	49.818714
653.741129	176.181798	49.823719
649.856705	180.938118	49.828724
646.226428	176.699945	49.833729
642.818479	162.074312	49.838733
639.548319	179.130960	49.843738
635.868703	179.377005	49.848743
632.647328	167.635509	49.853748
628.884403	167.421873	49.858753
625.635899	179.974525	49.863757
622.463977	176.215300	49.868762
618.610564	178.835969	49.873767
615.023689	173.670199	49.878772
611.254783	177.959173	49.883777
607.672883	178.318825	49.888781
604.420644	179.804335	49.893786
601.029204	187.282235	49.898791
597.959945	174.303559	49.903796
594.209734	172.319657	49.908801
590.534657	180.930594	49.913805
586.784522	178.913435	49.918810
583.103420	178.445199	49.923815
580.060868	170.230303	49.928820
576.362801	176.435206	49.933825
572.905287	172.740839	49.938829
569.622051	171.330350	49.943834
565.565523	178.583676	49.948839
562.911595	184.551508	49.953844
558.815688	176.651286	49.958849
555.481774	178.016436	49.963853
552.186231	165.441673	49.968858
548.542299	166.852606	49.973863
545.161628	168.480899	49.978868
541.075854	178.574401	49.983873
537.707437	164.259087	49.988877
534.291687	161.790041	49.993882
530.686407	165.655930	49.998887
527.544218	163.401952	50.003892
523.795878	165.852303	50.008897
520.519671	176.200790	50.013901
517.017200	178.972498	50.018906
513.293498	180.189945	50.023911
510.085731	176.603920	50.028916
506.399141	177.289610	50.033921
502.675492	161.456303	50.038925
499.437193	171.563243	50.043930
495.775832	172.039668	50.048935
492.550506	167.175428	50.053940
489.007421	172.860909	50.058945
485.724560	164.466652	50.063949
481.835185	163.798672	50.068954
478.157037	167.190061	50.073959
474.901955	160.618107	50.078964
471.381956	171.144307	50.083969
467.873936	187.669791	50.088973
464.467460	172.427829	50.093978
460.792852	167.165563	50.098983
457.224711	168.202161	50.103988
453.822211	172.097141	50.108993
450.324410	168.067070	50.113997
447.202921	168.708673	50.119002
443.397553	176.372315	50.124007
439.546955	161.180562	50.129012
436.039216	173.126560	50.134017
432.824300	164.429586	50.139021
429.448070	158.895686	50.144026
425.854836	165.275818	50.149031
422.598665	170.177480	50.154036
418.402649	164.982728	50.159041
415.217834	166.459558	50.164045
412.268182	159.917391	50.169050
408.221744	162.253283	50.174055
404.932071	178.040291	50.179060
401.155261	181.974245	50.184065
397.862949	171.518634	50.189069
394.344261	161.275442	50.194074
390.654978	172.653801	50.199079
387.269053	167.195416	50.204084
383.495128	161.413816	50.209089
379.941361	166.476236	50.214093
377.081402	175.061429	50.219098
373.646030	170.592239	50.224103
370.058084	166.389467	50.229108
366.295973	169.070467	50.234113
362.734707	174.174388	50.239117
359.225478	162.700126	50.244122
355.367880	180.825855	50.249127
352.161657	182.379060	50.254132
348.337247	175.926778	50.259137
345.102494	174.133016	50.264141
341.568380	163.107610	50.269146
338.068716	176.074079	50.274151
334.918888	165.544856	50.279156
331.156417	165.287418	50.284161
327.664273	172.945342	50.289165
324.492625	168.378254	50.294170
320.398249	170.229539	50.299175
317.251943	164.622398	50.304180
313.588051	175.253140	50.309185
310.104486	172.055020	50.314189
306.561318	160.622016	50.319194
303.325287	175.085527	50.324199
299.967125	165.711754	50.329204
296.275074	166.881672	50.334209
292.590812	166.937980	50.339213
289.776584	172.155780	50.344218
285.792371	165.742672	50.349223
282.142749	163.451804	50.354228
278.249171	159.602354	50.359233
275.181672	174.255563	50.364237
271.536206	159.604710	50.369242
267.900843	166.747374	50.374247
264.517076	158.153280	50.379252
261.335773	158.932217	50.384257
257.767018	164.580615	50.389261
254.353347	162.534903	50.394266
250.356460	168.086822	50.399271
247.342630	157.405952	50.404276
243.664751	174.672641	50.409281
239.921636	166.039176	50.414285
236.706562	156.726649	50.419290
232.946090	168.861184	50.424295
229.657530	163.682374	50.429300
226.246786	167.013340	50.434305
222.409825	164.453945	50.439309
219.086550	161.441700	50.444314
215.472393	170.945035	50.449319
212.115803	170.759017	50.454324
208.702272	167.156150	50.459329
205.107358	167.841858	50.464333
201.639279	168.839175	50.469338
198.110753	164.864743	50.474343
194.884678	163.966886	50.479348
191.375170	171.397681	50.484353
187.307069	167.686138	50.489357
184.299477	166.199329	50.494362
180.420249	171.654898	50.499367
177.276309	160.750310	50.504372
173.540242	161.079541	50.509377
169.920199	164.473924	50.514381
166.477094	161.833012	50.519386
162.910117	161.374674	50.524391
159.673597	154.906778	50.529396
156.192521	168.671413	50.534401
152.530922	167.744915	50.539405
149.483130	152.096072	50.544410
145.379298	165.314269	50.549415
141.951597	162.161968	50.554420
138.380570	162.694010	50.559425
135.094451	161.050021	50.564429
131.682817	166.021798	50.569434
127.924237	160.376439	50.574439
124.551152	163.946289	50.579444
121.160692	161.950682	50.584449
117.630292	160.131903	50.589453
114.154540	159.925082	50.594458
110.311447	163.425313	50.599463
106.908763	157.025353	50.604468
103.225265	163.208551	50.609473
99.857030	172.964997	50.614477
96.681704	170.438906	50.619482
92.833661	165.563152	50.624487
89.305934	150.505967	50.629492
86.035712	165.551828	50.634497
82.608854	175.721664	50.639501
79.301485	165.681120	50.644506
75.441976	155.582758	50.649511
72.018216	168.257201	50.654516
68.227284	173.162945	50.659521
64.959908	165.956545	50.664525
61.452715	161.282568	50.669530
57.992941	177.299354	50.674535
54.148199	160.749647	50.679540
50.962631	154.884853	50.684545
47.421418	162.858615	50.689549
44.322157	166.005510	50.694554
40.194039	166.600564	50.699559
36.894786	164.060554	50.704564
33.531388	165.912369	50.709569
29.823793	162.241395	50.714573
26.569242	157.026896	50.719578
22.936664	159.512656	50.724583
19.805416	151.208368	50.729588
16.109492	159.725150	50.734593
12.197455	167.922400	50.739597
8.688956	154.086288	50.744602
5.057508	149.204106	50.749607
1.773668	162.548690	50.754612