Thu Jun 16 11:32:04 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.620727	106.830623	0.000000
0.716516	107.334884	0.005005
0.485535	97.566360	0.010010
0.559822	107.628203	0.015014
0.506339	101.518716	0.020019
0.109530	80.803460	0.025024
0.268967	61.453917	0.030029
-0.385950	61.533028	0.035034
-0.600841	53.608470	0.040038
-0.807781	43.709337	0.045043
-1.050679	37.131595	0.050048
-1.156662	30.469277	0.055053
-1.677901	29.940791	0.060058
-2.122656	20.966188	0.065062
-1.896078	15.155741	0.070067
-2.579056	-0.270963	0.075072
-2.773548	-6.163251	0.080077
-2.995387	-7.073674	0.085082
-3.409705	-6.842836	0.090086
-3.371134	-11.894934	0.095091
-3.803804	0.155705	0.100096
-3.944101	-22.459439	0.105101
-4.665277	-14.370886	0.110106
-5.277538	1.845067	0.115110
-5.564666	4.257121	0.120115
-6.114518	-12.051036	0.125120
-5.453673	-2.780812	0.130125
-6.018981	-8.143318	0.135130
-6.159047	-2.328062	0.140134
-5.896022	-13.807703	0.145139
-6.331904	-0.237869	0.150144
-6.513436	-10.093122	0.155149
-7.070318	-8.391484	0.160154
-7.528836	-5.924176	0.165158
-7.590732	-7.276459	0.170163
-7.610467	-3.764217	0.175168
-7.494427	-12.686255	0.180173
-8.604804	-11.034915	0.185178
-8.941174	-13.459085	0.190182
-8.909939	-12.833965	0.195187
-9.123135	-13.718587	0.200192
-9.110926	-16.239624	0.205197
-9.894619	-12.513435	0.210202
-10.379318	-11.452836	0.215206
-10.223926	-17.173670	0.220211
-10.652437	-1.485594	0.225216
-10.439657	-5.911030	0.230221
-10.867445	-12.740737	0.235226
-10.995286	-7.537476	0.240230
-10.476411	-10.524129	0.245235
-11.667508	-5.482159	0.250240
-11.865491	-12.944424	0.255245
-12.416334	-9.494862	0.260250
-12.123965	-12.694268	0.265254
-12.407577	-7.756193	0.270259
-13.317784	-7.517199	0.275264
-13.703444	-11.661132	0.280269
-13.621901	-19.319342	0.285274
-13.694743	-6.320926	0.290278
-13.815657	-14.167848	0.295283
-13.960570	-8.034230	0.300288
-13.562447	-23.114731	0.305293
-14.434959	-15.393216	0.310298
-15.237989	-13.825122	0.315302
-15.128575	-16.072183	0.320307
-15.665675	-14.886218	0.325312
-15.344612	-14.248815	0.330317
-15.352703	-10.472433	0.335322
-16.205565	-9.169570	0.340326
-16.593390	-13.220904	0.345331
-16.947466	-7.338715	0.350336
-17.053167	-3.701481	0.355341
-17.261882	-9.600788	0.360346
-17.066347	-4.535216	0.365350
-17.282502	-15.787392	0.370355
-18.131596	-4.512313	0.375360
-18.403561	-13.370526	0.380365
-18.809038	-19.444484	0.385370
-18.897058	-8.384559	0.390374
-18.802052	-14.703117	0.395379
-19.029376	-10.627793	0.400384
-18.859774	-18.707105	0.405389
-19.294348	-11.704433	0.410394
-20.143720	-10.225064	0.415398
-20.091153	-12.670494	0.420403
-20.431413	-3.090407	0.425408
-20.285511	-18.745319	0.430413
-21.144343	-17.951407	0.435418
-21.915971	-13.078396	0.440422
-21.819126	-23.464620	0.445427
-21.797937	-3.624963	0.450432
-21.621801	-19.051162	0.455437
-21.692080	-16.006473	0.460442
-21.916618	-17.106159	0.465446
-22.591299	-24.516375	0.470451
-23.329262	-19.167701	0.475456
-23.520877	-15.796347	0.480461
-23.504013	-21.374916	0.485466
-23.665454	-16.403465	0.490470
-23.314396	-19.672746	0.495475
-24.103301	-20.260877	0.500480
-24.313814	-17.346617	0.505485
-24.798634	-15.080852	0.510490
-25.110383	-11.280926	0.515494
-25.161405	-17.909290	0.520499
-25.525249	-14.463502	0.525504
-25.257707	-14.608749	0.530509
-25.825786	-6.717937	0.535514
-26.884591	-13.328628	0.540518
-26.577098	-22.535343	0.545523
-27.016718	-5.301024	0.550528
-26.608965	-11.997315	0.555533
-26.860309	-11.155912	0.560538
-26.794946	-8.374746	0.565542
-27.341605	-15.347978	0.570547
-28.169987	-1.810259	0.575552
-28.253380	-11.182246	0.580557
-28.051575	-9.880536	0.585562
-28.613380	-13.402157	0.590566
-29.168663	-8.259073	0.595571
-29.814598	-10.266574	0.600576
-29.977183	-9.626688	0.605581
-29.979932	-13.623175	0.610586
-29.966292	-11.441066	0.615590
-30.049537	-11.125246	0.620595
-30.278613	0.102916	0.625600
-29.998969	-15.191819	0.630605
-30.229265	-11.706738	0.635610
-31.021617	-6.061793	0.640614
-30.909570	-17.748905	0.645619
-31.852135	-10.212820	0.650624
-32.471418	-7.508517	0.655629
-32.897909	-15.898632	0.660634
-32.422043	-10.408322	0.665638
-32.649047	-12.863684	0.670643
-33.183300	0.716683	0.675648
-33.198033	-16.772280	0.680653
-33.226062	-12.198348	0.685658
-33.263102	-8.676936	0.690662
-33.126602	-14.577057	0.695667
-34.225170	-3.070349	0.700672
-34.430963	-10.166799	0.705677
-34.679283	-6.856708	0.710682
-34.923978	-2.324904	0.715686
-35.624189	-5.820891	0.720691
-36.128787	-10.304362	0.725696
-35.546301	-7.486523	0.730701
-35.996066	-8.413635	0.735706
-36.629124	-9.113545	0.740710
-36.403105	-15.103239	0.745715
-36.665280	-0.067718	0.750720
-36.744366	-19.474118	0.755725
-36.806673	-7.719784	0.760730
-37.245513	0.380423	0.765734
-37.660915	-9.768046	0.770739
-38.199870	-8.540042	0.775744
-37.954656	-10.689287	0.780749
-37.849726	-6.803235	0.785754
-38.835167	-12.248130	0.790758
-38.907436	-16.726490	0.795763
-39.417021	-3.729099	0.800768
-39.414165	-11.742679	0.805773
-39.615021	-11.923279	0.810778
-39.787178	-5.717582	0.815782
-40.385192	-14.097799	0.820787
-40.891953	-17.518812	0.825792
-41.092074	-14.655102	0.830797
-41.071182	-8.757143	0.835802
-41.375777	-9.037700	0.840806
-41.042971	-19.874402	0.845811
-41.415153	-6.301094	0.850816
-41.392999	-10.307023	0.855821
-42.505611	-9.089579	0.860826
-42.773568	-12.450812	0.865830
-42.572226	-21.024290	0.870835
-42.843552	-14.166291	0.875840
-42.877749	-16.228518	0.880845
-43.700385	-16.717450	0.885850
-43.825592	-10.034930	0.890854
-44.165905	-12.132101	0.895859
-44.541289	-12.879526	0.900864
-44.231126	-14.351301	0.905869
-44.548274	-16.062226	0.910874
-44.675434	-7.058767	0.915878
-45.116142	-17.835709	0.920883
-45.846680	-4.089431	0.925888
-45.801912	-17.105132	0.930893
-46.079021	-13.625634	0.935898
-45.985274	-4.951878	0.940902
-46.036603	-19.415707	0.945907
-47.007703	-10.074291	0.950912
-47.333549	-16.819226	0.955917
-47.858331	-21.354799	0.960922
-48.125668	-2.947655	0.965926
-47.891685	-10.798572	0.970931
-48.054053	-8.543180	0.975936
-47.941987	-14.200522	0.980941
-47.863475	-12.813426	0.985946
-48.098858	-15.968134	0.990950
-49.015702	-17.528850	0.995955
-49.196373	-5.442126	1.000960
-49.817141	-14.457754	1.005965
-49.442140	-17.964209	1.010970
-49.670081	-0.424615	1.015974
-49.996700	-12.705044	1.020979
-50.828981	-5.879528	1.025984
-51.292816	-16.115088	1.030989
-51.314492	-17.326529	1.035994
-51.396624	-15.804860	1.040998
-51.404080	-3.718348	1.046003
-51.475720	-8.502441	1.051008
-51.450096	-9.137969	1.056013
-52.360042	-10.893777	1.061018
-52.993881	-5.202220	1.066022
-52.967224	-30.097870	1.071027
-53.268835	-4.819413	1.076032
-53.175754	-11.446042	1.081037
-52.818219	-9.277062	1.086042
-53.407808	-9.254023	1.091046
-54.095801	-11.008727	1.096051
-54.483592	-8.586845	1.101056
-54.285901	-17.402803	1.106061
-54.771684	-16.104072	1.111066
-54.653719	-6.732897	1.116070
-54.839563	-5.018485	1.121075
-55.453217	-9.118422	1.126080
-55.671626	-23.911758	1.131085
-55.564332	-9.879049	1.136090
-56.242735	-4.414230	1.141094
-56.968505	-13.483338	1.146099
-57.108733	-10.238169	1.151104
-57.451526	-10.135756	1.156109
-57.087383	-12.239446	1.161114
-57.411346	-8.064789	1.166118
-57.365640	-13.875520	1.171123
-57.848925	-0.367604	1.176128
-58.231162	-14.018009	1.181133
-58.781771	-12.933394	1.186138
-59.093941	-3.287119	1.191142
-58.948184	-14.293472	1.196147
-59.416713	-12.906140	1.201152
-59.183714	-10.338838	1.206157
-59.278301	-3.364332	1.211162
-60.265121	-18.356534	1.216166
-60.590843	-17.898734	1.221171
-60.677815	-12.872407	1.226176
-60.664803	-7.505576	1.231181
-60.463360	-13.066902	1.236186
-60.904287	-5.548406	1.241190
-61.575439	-19.668396	1.246195
-61.888936	-0.331315	1.251200
-62.075990	-6.681097	1.256205
-62.069038	-17.704266	1.261210
-62.570599	-9.088102	1.266214
-62.471559	-9.407939	1.271219
-63.003308	-7.790360	1.276224
-63.585184	-12.048853	1.281229
-63.640476	-12.507540	1.286234
-63.770509	-13.832874	1.291238
-63.717039	-9.036533	1.296243
-64.220938	-2.942931	1.301248
-64.273587	-9.643538	1.306253
-64.868640	-13.747828	1.311258
-65.371999	0.801235	1.316262
-65.128400	-12.384652	1.321267
-65.261536	-5.809734	1.326272
-65.617165	-7.010477	1.331277
-66.317056	-12.717029	1.336282
-66.712864	-9.932259	1.341286
-66.635912	-17.701778	1.346291
-66.686108	-19.807233	1.351296
-66.914764	-12.977792	1.356301
-66.940158	-9.192435	1.361306
-67.317410	-6.072549	1.366310
-67.364180	-22.318010	1.371315
-67.919157	-12.972756	1.376320
-68.336209	-19.864996	1.381325
-68.511199	-14.756152	1.386330
-68.855223	-9.237880	1.391334
-69.603767	-25.269694	1.396339
-69.544084	-3.040228	1.401344
-69.607848	-8.239767	1.406349
-70.156448	-12.699190	1.411354
-70.186102	-16.842166	1.416358
-69.998043	-13.007936	1.421363
-70.567217	-4.192563	1.426368
-70.075571	-12.544008	1.431373
-70.702907	-3.181660	1.436378
-71.663407	-6.172041	1.441382
-71.706782	-10.300025	1.446387
-71.919456	-19.365430	1.451392
-72.100033	-7.703328	1.456397
-71.902549	-15.595661	1.461402
-72.533754	-20.178065	1.466406
-73.253722	-19.392495	1.471411
-73.728532	-14.182802	1.476416
-73.498275	-12.285296	1.481421
-73.209163	-17.099408	1.486426
-73.979325	-2.903334	1.491430
-73.658257	-20.339460	1.496435
-74.150765	-14.202563	1.501440
-74.471556	-16.062047	1.506445
-74.573079	-19.980942	1.511450
-75.267946	-17.262075	1.516454
-75.790621	-13.671554	1.521459
-75.456107	-2.903430	1.526464
-75.534213	-11.618170	1.531469
-75.488644	-21.383478	1.536474
-76.313058	-13.824794	1.541478
-76.643234	-16.479941	1.546483
-76.688323	-15.132992	1.551488
-77.037415	-19.169607	1.556493
-77.110296	-17.582975	1.561498
-77.554100	-20.982128	1.566502
-78.172515	-10.712073	1.571507
-78.226599	-12.034864	1.576512
-78.554015	-20.464921	1.581517
-78.436322	-22.212783	1.586522
-78.724827	-13.531109	1.591526
-78.200310	-22.502490	1.596531
-79.412524	-15.107604	1.601536
-79.470531	-23.590470	1.606541
-79.868305	-15.542538	1.611546
-80.216376	-14.404480	1.616550
-80.015094	-24.870306	1.621555
-80.393211	-17.839578	1.626560
-80.898192	-4.598490	1.631565
-81.279786	-14.988611	1.636570
-81.561307	-8.251156	1.641574
-81.346599	-17.009550	1.646579
-81.601366	-7.662410	1.651584
-81.650836	-16.932955	1.656589
-82.580653	-11.345889	1.661594
-83.450765	-9.922179	1.666598
-83.275196	-11.155661	1.671603
-83.082035	-15.713598	1.676608
-83.203267	-10.216953	1.681613
-83.176606	-19.141475	1.686618
-83.717685	-15.434955	1.691622
-83.393899	-9.531121	1.696627
-84.077263	-5.329720	1.701632
-84.674999	-9.736036	1.706637
-84.611751	-14.331694	1.711642
-85.208727	-8.061316	1.716646
-85.615858	-15.538728	1.721651
-86.068494	-5.522871	1.726656
-85.694379	-8.446734	1.731661
-85.997557	-13.947845	1.736666
-86.787744	-8.634039	1.741670
-86.774538	-15.390806	1.746675
-87.078191	-13.457054	1.751680
-86.792460	-18.616386	1.756685
-86.750098	-21.290087	1.761690
-87.495566	-3.508904	1.766694
-87.935646	-8.674464	1.771699
-88.322528	-6.232902	1.776704
-88.134874	-8.207983	1.781709
-88.297318	-13.130767	1.786714
-88.530443	-10.992226	1.791718
-89.277066	-14.459914	1.796723
-90.162645	-10.959862	1.801728
-89.997772	-11.978486	1.806733
-89.999569	-20.930464	1.811738
-90.271716	-9.839920	1.816742
-90.076057	-20.111558	1.821747
-90.514211	-9.648239	1.826752
-90.447847	-6.184266	1.831757
-90.652193	-18.881969	1.836762
-91.502324	-13.473613	1.841766
-91.621687	-19.748351	1.846771
-91.670746	-19.090429	1.851776
-91.664977	-15.537423	1.856781
-91.857239	-17.780499	1.861786
-92.547319	-10.701368	1.866790
-92.877536	-29.226506	1.871795
-93.289548	-14.578316	1.876800
-93.584545	-25.423817	1.881805
-93.465811	-24.930063	1.886810
-93.580489	-18.167309	1.891814
-94.593966	-13.555117	1.896819
-94.885719	-20.684111	1.901824
-95.079022	-16.549497	1.906829
-94.853678	-16.519865	1.911834
-95.143682	-11.277871	1.916838
-94.676046	-18.192115	1.921843
-94.949733	-15.940325	1.926848
-95.974254	-14.716418	1.931853
-96.371759	-15.966963	1.936858
-96.825185	-0.236499	1.941862
-96.532837	-8.095779	1.946867
-96.642572	-15.209674	1.951872
-96.804923	-19.301517	1.956877
-97.102063	-14.426418	1.961882
-98.376511	4.376933	1.966886
-98.220750	-8.413538	1.971891
-98.622326	-13.393578	1.976896
-98.669779	-6.536962	1.981901
-98.438253	-18.118129	1.986906
-98.698983	-13.120010	1.991910
-98.928020	-15.235961	1.996915
-98.699890	-16.993758	2.006912
-99.250291	-13.105103	2.016909
-98.623530	-14.665311	2.026906
-98.156780	-10.247772	2.036902
-97.188669	-13.185469	2.046899
-96.888405	-13.137524	2.056896
-96.858747	-22.899816	2.066893
-96.191714	-9.948697	2.076890
-95.354456	-20.358706	2.086886
-95.316248	-15.556176	2.096883
-94.322095	-17.608520	2.106880
-94.019141	-19.070219	2.116877
-93.863755	-18.694684	2.126874
-92.917859	-15.135157	2.136870
-92.709015	-14.477650	2.146867
-92.064114	-18.206986	2.156864
-91.156683	-18.112057	2.166861
-91.119368	-20.594991	2.176858
-90.986852	-14.363005	2.186854
-90.114185	-22.706376	2.196851
-89.856222	-4.947378	2.206848
-88.535096	-17.884762	2.216845
-88.357217	-12.862316	2.226842
-88.152080	-8.820512	2.236838
-87.745292	-13.027359	2.246835
-86.962535	-14.718053	2.256832
-86.591969	-13.960342	2.266829
-85.832994	-12.251914	2.276826
-85.008335	-17.576708	2.286822
-85.149076	-10.121321	2.296819
-84.838481	-9.213036	2.306816
-84.123602	-12.041563	2.316813
-83.564897	-9.925020	2.326810
-83.174005	-17.231898	2.336806
-81.976959	-24.819676	2.346803
-82.001187	-14.695418	2.356800
-81.967872	-11.755746	2.366797
-80.902267	-10.905463	2.376794
-80.602135	-8.373493	2.386790
-79.933099	-7.958926	2.396787
-79.522366	-6.915021	2.406784
-79.115239	-11.924112	2.416781
-78.776941	-9.292163	2.426778
-77.373063	-14.673516	2.436774
-77.350373	-14.834844	2.446771
-77.140405	-10.410475	2.456768
-76.591276	-21.273183	2.466765
-75.878657	-11.023204	2.476762
-75.683700	-17.136402	2.486758
-75.239749	-3.680487	2.496755
-74.418188	-15.435156	2.506752
-74.186861	-16.805698	2.516749
-72.961542	-10.809577	2.526746
-72.667963	-20.409534	2.536742
-72.501200	-14.841768	2.546739
-72.473235	-22.993531	2.556736
-71.457222	-9.961049	2.566733
-70.943146	-14.408374	2.576730
-70.629970	-14.011994	2.586726
-69.826639	-14.434699	2.596723
-69.400183	-5.811436	2.606720
-69.263131	-12.826552	2.616717
-68.091403	-12.630290	2.626714
-67.827094	-8.913764	2.636710
-67.611865	-10.522667	2.646707
-67.397090	-11.442755	2.656704
-66.484918	-10.970479	2.666701
-66.140225	-11.269479	2.676698
-64.929690	-9.668468	2.686694
-64.600925	-14.633640	2.696691
-64.895996	-9.562319	2.706688
-64.043221	-11.246506	2.716685
-63.231264	-12.848677	2.726682
-63.035514	-19.500995	2.736678
-62.564842	-18.317640	2.746675
-61.700436	-17.123839	2.756672
-61.392956	-12.552845	2.766669
-61.177509	-10.319663	2.776666
-60.258905	-15.060193	2.786662
-60.309752	-12.295774	2.796659
-59.723765	-8.190865	2.806656
-58.543669	-11.930908	2.816653
-58.155671	-14.766951	2.826650
-58.361853	-3.887869	2.836646
-57.118171	-10.178582	2.846643
-56.980165	-11.264527	2.856640
-56.838790	-18.735679	2.866637
-55.529741	-12.989474	2.876634
-55.138719	-12.075168	2.886630
-55.212513	-17.433037	2.896627
-54.907512	-11.968915	2.906624
-54.065258	-11.399588	2.916621
-53.382575	-14.220717	2.926618
-52.380662	-10.697011	2.936614
-52.273176	-15.464752	2.946611
-52.080246	-7.583992	2.956608
-51.803905	-9.255890	2.966605
-50.948830	-8.245854	2.976602
-50.272337	-17.993206	2.986598
-50.092422	-10.233573	2.996595
-49.098668	-7.120377	3.006592
-48.998448	-12.399583	3.016589
-48.736350	-13.929848	3.026586
-47.703875	-12.658224	3.036582
-47.216434	-9.771226	3.046579
-47.316117	-10.957268	3.056576
-46.212144	-2.455646	3.066573
-45.803436	-9.902084	3.076570
-45.705313	-12.320096	3.086566
-44.674624	-20.480020	3.096563
-44.118460	-10.154641	3.106560
-44.055787	-14.075253	3.116557
-43.775586	-13.735456	3.126554
-42.350409	-15.581850	3.136550
-42.237171	-18.012730	3.146547
-42.019458	-13.574872	3.156544
-41.798446	-13.494368	3.166541
-41.061396	-16.992623	3.176538
-40.269456	-21.229681	3.186534
-39.427521	-13.667070	3.196531
-39.305270	-8.944853	3.206528
-39.446550	-18.974106	3.216525
-38.139649	-13.930258	3.226522
-37.874185	-14.134769	3.236518
-37.490959	-12.870878	3.246515
-36.787571	-19.434520	3.256512
-36.008558	-13.817933	3.266509
-36.000328	-10.307071	3.276506
-35.875969	-9.416507	3.286502
-34.953703	-9.896694	3.296499
-34.476139	-6.233977	3.306496
-33.544646	-9.959654	3.316493
-33.170653	-16.139087	3.326490
-32.853618	-17.483292	3.336486
-32.755746	-14.548756	3.346483
-32.286136	-12.909257	3.356480
-31.597726	-7.950826	3.366477
-30.360613	-11.997120	3.376474
-29.767888	-18.102363	3.386470
-30.081536	-11.224114	3.396467
-29.804150	-3.864193	3.406464
-28.730355	-9.165407	3.416461
-28.128219	-15.116679	3.426458
-28.262343	-12.795500	3.436454
-27.251846	-11.648109	3.446451
-26.891049	-13.018463	3.456448
-26.853673	-13.172636	3.466445
-25.783406	-14.061285	3.476442
-25.132496	-15.307903	3.486438
-25.196295	-12.621848	3.496435
-23.722360	-16.723278	3.506432
-23.423825	-7.616335	3.516429
-23.492303	-13.209243	3.526426
-23.237513	-17.692542	3.536422
-22.363954	-13.899782	3.546419
-22.155360	-11.131464	3.556416
-21.099964	-14.894011	3.566413
-20.431436	-12.075312	3.576410
-20.202802	-19.659122	3.586406
-20.038464	-10.497110	3.596403
-19.539260	-11.065428	3.606400
-18.664151	-12.953823	3.616397
-18.297840	-15.926695	3.626394
-18.179645	-15.920867	3.636390
-17.078031	-7.239912	3.646387
-16.985319	-8.799032	3.656384
-16.740969	-12.175415	3.666381
-15.689039	-3.913320	3.676378
-15.188502	-10.163798	3.686374
-14.886817	-7.249211	3.696371
-13.731472	-9.353421	3.706368
-13.692305	-5.335300	3.716365
-13.636941	-13.371140	3.726362
-13.079855	-11.492233	3.736358
-12.333202	-11.264980	3.746355
-12.019126	-8.547134	3.756352
-11.086592	-9.183654	3.766349
-10.499021	-9.141993	3.776346
-10.353473	-5.751317	3.786342
-10.007630	-11.140557	3.796339
-9.218265	-15.741141	3.806336
-8.674956	-16.976741	3.816333
-8.705392	-12.826461	3.826330
-7.560992	-20.694661	3.836326
-6.872895	-17.671906	3.846323
-7.029754	-12.783498	3.856320
-6.571627	-23.731774	3.866317
-5.778463	-16.615977	3.876314
-5.847027	-21.288195	3.886310
-4.822785	-22.357261	3.896307
-4.401595	-12.229157	3.906304
-3.900530	2.219654	3.916301
-3.476612	11.260157	3.926298
-3.050547	0.719688	3.936294
-2.623541	21.412260	3.946291
-2.202565	38.596954	3.956288
-1.807482	48.270483	3.966285
-1.502562	75.134864	3.976282
-0.682643	89.615672	3.986278
-0.370572	105.807820	3.996275
0.000000	127.112100	4.001280
0.140981	140.682129	4.006285
0.407274	135.615732	4.011290
0.324403	155.487594	4.016294
0.913310	157.877728	4.021299
0.485467	163.878126	4.026304
0.647427	163.728722	4.031309
0.728326	165.850711	4.036314
0.671282	164.656840	4.041318
0.952027	166.152201	4.046323
0.895005	158.689543	4.051328
0.918475	163.408524	4.056333
0.788725	165.734910	4.061338
0.681754	180.393162	4.066342
1.051648	183.512935	4.071347
1.007291	201.147325	4.076352
0.995426	198.649369	4.081357
0.990289	194.111116	4.086362
1.179977	195.597161	4.091366
1.507378	196.272002	4.096371
1.191276	204.837018	4.101376
1.495449	185.066811	4.106381
1.208236	183.276133	4.111386
0.831608	165.717918	4.116390
1.244816	181.550617	4.121395
1.068350	189.269280	4.126400
1.324230	179.836372	4.131405
1.328216	171.708364	4.136410
1.190156	178.791261	4.141414
1.126223	157.178681	4.146419
1.089547	172.288195	4.151424
1.181886	186.814074	4.156429
1.649493	191.373544	4.161434
1.565102	185.407937	4.166438
1.585414	167.732528	4.171443
1.071845	177.154220	4.176448
1.022168	164.637865	4.181453
1.269093	170.373252	4.186458
0.930488	174.823453	4.191462
1.532326	178.568148	4.196467
1.371038	174.800052	4.201472
1.336416	193.032049	4.206477
1.707585	195.021330	4.211482
1.314152	184.376909	4.216486
1.349690	167.453097	4.221491
1.122822	185.827447	4.226496
1.270007	198.311698	4.231501
1.388822	196.704010	4.236506
1.212146	192.909152	4.241510
1.472893	204.562421	4.246515
1.091200	203.309137	4.251520
1.703889	198.768525	4.256525
1.656108	205.124132	4.261530
1.385532	200.827444	4.266534
1.575498	201.254289	4.271539
1.344314	210.497633	4.276544
1.256428	203.274161	4.281549
1.498374	200.084623	4.286554
1.290504	206.460864	4.291558
1.607119	207.169946	4.296563
1.316412	205.556730	4.301568
1.574230	197.186889	4.306573
1.743727	205.603785	4.311578
1.491977	205.078605	4.316582
1.541490	202.634434	4.321587
1.297489	222.504597	4.326592
1.659425	224.733461	4.331597
1.852370	229.279138	4.336602
1.469452	237.076237	4.341606
2.336774	227.247182	4.346611
1.782270	222.104979	4.351616
1.697098	221.960701	4.356621
1.974797	204.412006	4.361626
1.561823	203.388824	4.366630
1.874650	205.840769	4.371635
1.702504	209.729850	4.376640
1.948341	213.438873	4.381645
2.004155	208.482212	4.386650
1.817653	212.218186	4.391654
1.858274	197.825864	4.396659
1.774984	204.102693	4.401664
1.565815	209.407170	4.406669
2.052793	219.632234	4.411674
1.859022	228.467192	4.416678
2.217100	228.068338	4.421683
1.790312	221.915031	4.426688
1.970032	206.210200	4.431693
1.510015	213.151968	4.436698
1.851981	224.693866	4.441702
1.782931	227.940049	4.446707
1.905902	241.620282	4.451712
2.341336	237.052718	4.456717
1.977356	228.785317	4.461722
2.076403	238.584088	4.466726
1.998755	239.509265	4.471731
1.933647	241.899464	4.476736
2.244115	233.376866	4.481741
2.438920	236.226167	4.486746
2.050484	252.541440	4.491750
2.221225	224.700879	4.496755
2.223310	236.398988	4.501760
2.138930	226.900540	4.506765
1.750696	223.565146	4.511770
1.807875	235.565799	4.516774
2.063908	229.581804	4.521779
2.199912	232.148309	4.526784
2.152947	233.269968	4.531789
2.031470	236.810225	4.536794
2.137948	228.474846	4.541798
2.018168	224.168524	4.546803
2.049880	239.741135	4.551808
2.252778	242.958068	4.556813
1.981328	232.310325	4.561818
2.071414	251.529639	4.566822
2.227367	235.861657	4.571827
2.249735	243.210879	4.576832
2.167759	241.420315	4.581837
2.272733	235.683154	4.586842
2.227939	243.108093	4.591846
2.344691	239.511568	4.596851
2.140021	244.234337	4.601856
2.287944	254.643803	4.606861
2.213685	268.340572	4.611866
2.176326	276.491386	4.616870
2.703827	274.882154	4.621875
2.487296	283.507514	4.626880
2.534350	278.073802	4.631885
2.814078	271.042500	4.636890
2.156983	275.529378	4.641894
2.682910	267.192538	4.646899
2.538281	267.917961	4.651904
2.636291	261.382442	4.656909
2.761441	249.858205	4.661914
2.309169	238.666463	4.666918
2.188076	245.942318	4.671923
2.171301	258.078134	4.676928
2.584805	263.235732	4.681933
2.645867	263.437836	4.686938
2.509821	275.942318	4.691942
2.727407	272.094126	4.696947
3.056719	270.676974	4.701952
2.918142	272.465882	4.706957
2.606300	261.463125	4.711962
2.288685	249.134127	4.716966
2.371267	264.375163	4.721971
2.593793	278.783032	4.726976
2.623824	271.162095	4.731981
2.709357	279.853751	4.736986
2.202276	281.678203	4.741990
2.609550	268.136994	4.746995
2.601019	274.976951	4.752000
2.578721	281.570378	4.757005
2.772880	281.082100	4.762010
2.691262	276.670703	4.767014
2.571063	276.514849	4.772019
2.707192	272.977661	4.777024
2.734969	272.450779	4.782029
2.641556	272.479916	4.787034
2.463500	274.930615	4.792038
2.889158	280.379117	4.797043
3.095707	298.531234	4.802048
2.586776	297.721311	4.807053
3.050023	301.856331	4.812058
2.807550	303.900664	4.817062
2.973721	298.013869	4.822067
3.089667	304.432039	4.827072
3.070215	294.084647	4.832077
2.846139	287.119919	4.837082
2.808162	288.531424	4.842086
2.945797	304.137305	4.847091
2.808892	301.635135	4.852096
2.961428	301.537996	4.857101
3.101668	304.721691	4.862106
2.863683	306.521407	4.867110
3.028610	299.320830	4.872115
2.808358	303.030932	4.877120
3.012379	304.386959	4.882125
2.927082	302.672506	4.887130
2.434997	311.991877	4.892134
2.973536	303.414090	4.897139
2.906711	299.450405	4.902144
2.942860	303.665278	4.907149
2.959943	300.954755	4.912154
2.823455	317.486050	4.917158
3.276663	322.283922	4.922163
3.470879	331.302743	4.927168
3.277340	326.512740	4.932173
3.183535	307.791340	4.937178
3.020708	311.787230	4.942182
2.874130	312.749255	4.947187
3.180599	333.952189	4.952192
3.195409	333.245034	4.957197
3.271384	322.365097	4.962202
3.346630	330.334254	4.967206
3.448925	339.371427	4.972211
3.342424	338.765808	4.977216
3.177719	335.375002	4.982221
3.365945	337.480561	4.987226
3.181016	329.558604	4.992230
3.494880	327.247914	4.997235
3.252966	337.235981	5.002240
3.317869	345.848608	5.007245
3.339863	338.894691	5.012250
3.140635	329.456299	5.017254
3.286245	328.022341	5.022259
3.401568	337.623148	5.027264
3.073883	330.317996	5.032269
3.184718	335.048539	5.037274
3.113692	337.449793	5.042278
3.400566	331.425146	5.047283
3.264822	325.563667	5.052288
3.108437	345.700282	5.057293
3.401293	342.763147	5.062298
3.680835	360.158919	5.067302
3.783516	364.453084	5.072307
3.946217	365.903156	5.077312
3.779906	347.198820	5.082317
3.721012	320.347170	5.087322
3.311057	340.483852	5.092326
3.678610	335.167633	5.097331
3.431971	330.413336	5.102336
3.183715	330.665471	5.107341
3.483728	343.744732	5.112346
3.466108	358.279276	5.117350
3.191869	366.243657	5.122355
3.448298	360.142146	5.127360
3.595198	363.788926	5.132365
3.884431	355.788994	5.137370
3.292779	371.431109	5.142374
3.656630	366.927919	5.147379
3.824652	352.961012	5.152384
3.807769	357.586190	5.157389
3.812769	366.468093	5.162394
3.531240	362.933508	5.167398
3.570633	366.231155	5.172403
3.817372	363.779919	5.177408
3.704330	363.011217	5.182413
4.007726	366.009523	5.187418
3.394513	375.627947	5.192422
3.764013	368.160703	5.197427
3.787461	387.942685	5.202432
3.836528	404.401877	5.207437
4.131792	389.822665	5.212442
4.408904	393.954532	5.217446
3.865785	379.706352	5.222451
3.919713	371.213937	5.227456
4.372431	363.328950	5.232461
3.944634	361.253579	5.237466
3.708678	372.766490	5.242470
3.456898	361.571222	5.247475
3.395125	375.534761	5.252480
3.612049	386.280971	5.257485
4.417191	400.331140	5.262490
4.105639	399.915675	5.267494
4.235761	397.326940	5.272499
3.901146	397.961431	5.277504
3.989176	406.227639	5.282509
4.080033	396.461677	5.287514
3.958979	402.557480	5.292518
4.146376	401.284424	5.297523
4.045195	395.014889	5.302528
3.835366	404.194245	5.307533
4.357536	397.721267	5.312538
4.021342	406.503305	5.317542
3.866954	400.429809	5.322547
3.908020	403.430629	5.327552
4.178795	407.251104	5.332557
4.364330	404.641274	5.337562
4.285181	405.121969	5.342566
4.070793	401.542835	5.347571
4.453840	406.009105	5.352576
4.082185	421.513990	5.357581
4.276379	404.187426	5.362586
4.320364	414.755452	5.367590
4.362533	402.174892	5.372595
4.289882	408.159109	5.377600
4.270342	408.176631	5.382605
4.513532	400.710514	5.387610
4.364823	406.019176	5.392614
4.443257	398.127160	5.397619
4.476407	403.369562	5.402624
4.301756	409.770291	5.407629
4.339319	403.689342	5.412634
4.314097	410.556683	5.417638
4.196355	404.279522	5.422643
4.151127	395.092665	5.427648
3.894388	404.679625	5.432653
4.402138	410.941344	5.437658
4.383023	417.349225	5.442662
4.863083	421.920123	5.447667
4.745452	426.026270	5.452672
4.373777	418.536262	5.457677
4.376865	409.051266	5.462682
4.371185	421.644029	5.467686
4.688516	416.001638	5.472691
4.653017	422.131257	5.477696
4.598248	418.608021	5.482701
4.649973	413.132547	5.487706
4.237787	405.309568	5.492710
4.745110	414.938579	5.497715
4.653079	416.070459	5.502720
4.737344	425.724105	5.507725
4.876972	418.646927	5.512730
4.611012	412.145643	5.517734
4.351813	409.150852	5.522739
4.330797	413.963388	5.527744
4.491779	425.373747	5.532749
4.851137	428.480218	5.537754
4.821158	435.360194	5.542758
5.023299	432.054755	5.547763
4.972086	434.495074	5.552768
4.831868	434.451245	5.557773
4.964094	428.995217	5.562778
4.665915	415.991321	5.567782
4.719156	413.974963	5.572787
4.698343	404.729115	5.577792
4.676929	429.810460	5.582797
5.051553	434.409736	5.587802
4.775104	431.328804	5.592806
4.691071	433.133677	5.597811
4.466305	436.483674	5.602816
4.820903	433.052905	5.607821
4.971472	434.180016	5.612826
4.979436	433.935204	5.617830
4.884971	436.675581	5.622835
5.322719	432.291077	5.627840
4.734677	436.698616	5.632845
4.940733	431.298360	5.637850
4.955155	442.692996	5.642854
4.654457	436.382324	5.647859
5.062262	442.349410	5.652864
4.850392	434.474372	5.657869
5.039468	418.348491	5.662874
5.112728	437.322897	5.667878
5.032291	435.437642	5.672883
5.238624	434.094170	5.677888
5.219041	422.984004	5.682893
5.359958	437.617027	5.687898
5.142510	438.513031	5.692902
5.050282	430.030036	5.697907
5.197625	437.324959	5.702912
4.831265	434.411110	5.707917
5.318979	423.389858	5.712922
4.861336	440.311858	5.717926
4.903452	436.125425	5.722931
5.211867	429.922558	5.727936
5.096163	434.625652	5.732941
4.867146	426.669396	5.737946
4.727662	431.429594	5.742950
4.759937	437.677456	5.747955
5.084608	439.781199	5.752960
5.264356	461.770032	5.757965
5.481302	462.573437	5.762970
5.194395	455.992133	5.767974
5.271781	464.239314	5.772979
5.581790	466.175204	5.777984
5.249034	452.476237	5.782989
5.379340	437.939334	5.787994
5.281823	445.144794	5.792998
5.243620	447.537485	5.798003
5.029148	445.683059	5.803008
4.859760	471.609546	5.808013
5.271161	456.141524	5.813018
5.276100	466.234498	5.818022
5.603063	469.343962	5.823027
5.580789	464.389765	5.828032
5.639404	466.862748	5.833037
5.586699	468.525218	5.838042
5.621366	473.386974	5.843046
5.636509	472.016986	5.848051
5.455549	454.400355	5.853056
5.245314	468.029699	5.858061
5.505899	468.425546	5.863066
5.305418	463.758191	5.868070
5.270610	457.970548	5.873075
5.563666	469.124313	5.878080
5.062800	465.196598	5.883085
5.313169	461.405588	5.888090
5.140478	461.638430	5.893094
5.440070	475.200302	5.898099
5.678801	478.810724	5.903104
5.857807	493.772839	5.908109
5.583536	472.999608	5.913114
5.536247	467.735619	5.918118
5.724630	472.485354	5.923123
5.697766	487.597503	5.928128
5.466972	501.838490	5.933133
5.626945	493.034291	5.938138
5.527309	499.932911	5.943142
5.379364	505.999458	5.948147
5.645001	496.343655	5.953152
5.290707	507.604523	5.958157
5.566673	499.564385	5.963162
5.385838	502.863234	5.968166
5.440616	499.478642	5.973171
5.694439	500.688042	5.978176
5.742864	522.756180	5.983181
6.038917	521.697298	5.988186
5.839219	521.597889	5.993190
5.470609	514.738432	5.998195
6.007470	517.190896	6.003200
5.731392	533.371484	6.008205
5.978542	531.421230	6.013210
6.136983	535.811890	6.018214
5.769658	535.637183	6.023219
5.958835	529.111347	6.028224
5.553925	530.725675	6.033229
6.131628	532.212647	6.038234
6.089482	531.306434	6.043238
5.772741	513.645580	6.048243
5.906456	506.255315	6.053248
5.723289	506.851366	6.058253
6.011488	492.270561	6.063258
5.697206	502.222254	6.068262
5.623030	509.715613	6.073267
5.845248	514.844234	6.078272
6.169535	521.849504	6.083277
6.231265	527.756807	6.088282
5.977374	517.194557	6.093286
6.023387	502.467797	6.098291
5.634765	499.227608	6.103296
5.690029	501.182120	6.108301
5.977385	487.077871	6.113306
5.846601	503.756901	6.118310
5.875499	496.894115	6.123315
5.823862	496.779019	6.128320
5.450927	506.543982	6.133325
5.765966	515.888736	6.138330
6.059807	529.692131	6.143334
6.159927	526.997049	6.148339
5.883958	511.514800	6.153344
5.617236	516.239225	6.158349
5.944081	493.625641	6.163354
6.182180	504.910650	6.168358
6.233185	503.405197	6.173363
6.211585	501.106311	6.178368
6.046161	489.208848	6.183373
5.968920	498.947731	6.188378
6.022282	501.546191	6.193382
5.923990	492.016927	6.198387
5.973785	500.179305	6.203392
5.979671	494.927829	6.208397
5.946430	493.320772	6.213402
6.029770	492.705677	6.218406
6.054329	500.892548	6.223411
5.820171	489.051430	6.228416
6.002370	504.611576	6.233421
6.151480	490.523658	6.238426
5.722944	491.799647	6.243430
5.824887	495.135722	6.248435
6.531542	491.184557	6.253440
6.127288	487.165498	6.258445
5.813646	476.801781	6.263450
5.919400	461.412281	6.268454
5.665053	466.251651	6.273459
5.918134	468.425732	6.278464
5.540799	469.350034	6.283469
5.761906	466.247841	6.288474
5.781076	477.481994	6.293478
6.270958	477.088781	6.298483
5.901257	467.884468	6.303488
5.596218	462.072617	6.308493
5.919354	471.300677	6.313498
5.736382	476.078139	6.318502
5.421525	477.308704	6.323507
5.577952	493.704177	6.328512
5.574574	499.451356	6.333517
5.897336	494.536517	6.338522
5.990609	505.253325	6.343526
6.097950	503.927883	6.348531
5.982590	498.196353	6.353536
5.912376	503.684063	6.358541
6.074726	509.506066	6.363546
5.948999	497.417548	6.368550
5.959961	501.903503	6.373555
5.885192	493.186536	6.378560
6.059113	485.794274	6.383565
6.227975	474.555852	6.388570
5.864657	483.818827	6.393574
5.809194	475.270144	6.398579
6.163159	470.244595	6.403584
5.814057	474.596282	6.408589
6.026917	472.958326	6.413594
5.966409	472.213691	6.418598
5.608519	468.456306	6.423603
5.876399	462.437509	6.428608
5.985923	478.270287	6.433613
6.023700	464.030807	6.438618
5.704965	471.296710	6.443622
5.813018	474.008954	6.448627
5.943716	462.875503	6.453632
5.834791	464.501289	6.458637
5.648706	470.477639	6.463642
5.843298	466.460254	6.468646
5.759687	468.103760	6.473651
5.825070	469.435653	6.478656
5.746778	465.897844	6.483661
6.011064	472.358756	6.488666
5.542894	471.812208	6.493670
5.638502	459.004641	6.498675
5.897354	476.576711	6.503680
5.616624	477.583015	6.508685
6.021289	485.752842	6.513690
6.073444	499.133648	6.518694
5.861543	487.785588	6.523699
5.799091	466.484180	6.528704
5.681567	476.021246	6.533709
6.030175	485.347313	6.538714
5.873206	489.098205	6.543718
5.998398	473.676969	6.548723
6.079224	464.241640	6.553728
5.703659	471.915407	6.558733
5.428191	461.592057	6.563738
5.681420	476.490588	6.568742
5.958246	498.167561	6.573747
6.427555	484.179751	6.578752
6.066045	481.909120	6.583757
5.993554	471.500524	6.588762
5.761255	462.599271	6.593766
6.124948	468.094780	6.598771
5.956319	467.768458	6.603776
5.605659	463.450401	6.608781
5.779085	461.603497	6.613786
5.990932	467.416023	6.618790
5.790404	475.929337	6.623795
5.984060	457.502292	6.628800
5.529541	458.016113	6.633805
5.649471	459.199886	6.638810
5.761754	460.938976	6.643814
5.798626	473.812628	6.648819
6.307449	471.260943	6.653824
5.573357	470.397948	6.658829
6.031877	461.722801	6.663834
5.754977	474.192810	6.668838
5.574467	450.298123	6.673843
6.168821	466.846727	6.678848
5.928687	470.455777	6.683853
5.810387	468.060803	6.688858
5.736666	454.239709	6.693862
5.735617	482.039596	6.698867
5.954002	479.704607	6.703872
5.895678	481.406286	6.708877
5.864933	488.007610	6.713882
6.010006	478.277921	6.718886
5.585118	486.977880	6.723891
5.974309	488.055203	6.728896
5.749214	495.419493	6.733901
5.954747	496.569786	6.738906
6.099998	485.449403	6.743910
5.811107	483.631935	6.748915
6.168629	470.818862	6.753920
5.580304	474.372688	6.758925
5.841093	473.021793	6.763930
6.154041	471.785401	6.768934
5.627755	458.245677	6.773939
5.916294	467.451434	6.778944
5.638189	479.029103	6.783949
5.665453	480.557999	6.788954
6.266757	494.570907	6.793958
5.655402	498.964361	6.798963
5.898504	483.480616	6.803968
5.644159	494.712724	6.808973
6.230725	501.956898	6.813978
5.951574	488.897903	6.818982
5.916361	480.846157	6.823987
5.899769	470.160966	6.828992
5.807282	473.101393	6.833997
5.839063	459.633314	6.839002
5.897169	471.990542	6.844006
5.602786	466.821548	6.849011
6.094707	478.687805	6.854016
5.897331	473.631722	6.859021
5.851355	468.296187	6.864026
5.800413	475.121537	6.869030
5.702982	469.085266	6.874035
6.035058	476.439358	6.879040
5.714330	483.048645	6.884045
6.077185	469.508286	6.889050
6.025384	475.397630	6.894054
5.882186	477.948261	6.899059
6.066974	468.479965	6.904064
5.758189	459.390982	6.909069
6.378781	466.243969	6.914074
6.042627	467.765142	6.919078
5.813450	454.454336	6.924083
6.221803	463.272501	6.929088
5.735491	479.180361	6.934093
6.154036	467.280136	6.939098
6.243365	470.063250	6.944102
5.831674	462.764123	6.949107
5.957793	471.998794	6.954112
5.511038	465.705833	6.959117
5.773591	463.120361	6.964122
5.762751	462.586733	6.969126
5.551845	464.282350	6.974131
5.808700	466.013828	6.979136
5.380435	473.116107	6.984141
5.818366	459.821040	6.989146
5.684158	475.132048	6.994150
6.044426	481.659776	6.999155
5.896792	471.107524	7.004160
5.824000	461.635627	7.009165
5.885924	474.122452	7.014170
6.073044	470.713925	7.019174
6.066742	461.386621	7.024179
6.324127	468.232049	7.029184
5.910262	472.379861	7.034189
5.867448	476.163285	7.039194
5.784122	463.785137	7.044198
5.854237	476.972845	7.049203
6.217028	463.371828	7.054208
5.996730	477.536672	7.059213
5.976903	471.273787	7.064218
5.867415	468.156970	7.069222
5.758730	472.457384	7.074227
5.951664	462.636727	7.079232
5.796958	467.277118	7.084237
5.729515	455.455436	7.089242
5.914031	466.863319	7.094246
5.696118	471.020481	7.099251
5.893886	463.150542	7.104256
5.829456	473.464135	7.109261
6.005771	473.475731	7.114266
5.809837	478.387140	7.119270
5.292302	461.983258	7.124275
6.107838	470.049170	7.129280
5.688150	471.029602	7.134285
5.988178	468.742487	7.139290
5.896974	470.220222	7.144294
5.715890	467.819444	7.149299
5.695276	459.231665	7.154304
5.680563	466.004360	7.159309
5.893626	471.732927	7.164314
5.664636	471.888649	7.169318
5.818779	479.753688	7.174323
6.094701	466.505513	7.179328
6.190177	470.686161	7.184333
5.912230	473.071316	7.189338
5.761575	461.500452	7.194342
5.943950	454.888263	7.199347
5.923557	463.552639	7.204352
5.787751	480.325803	7.209357
6.054039	459.931090	7.214362
6.067257	464.675930	7.219366
5.956536	463.107133	7.224371
6.105234	462.593312	7.229376
5.849180	470.977779	7.234381
6.023270	474.682049	7.239386
6.028614	463.057090	7.244390
5.812770	473.512415	7.249395
5.824597	471.730394	7.254400
5.721519	469.133421	7.259405
5.555829	467.872636	7.264410
6.235029	462.028759	7.269414
5.910626	474.525066	7.274419
5.945666	478.341895	7.279424
5.573166	473.218463	7.284429
5.903556	474.652772	7.289434
5.758027	467.626740	7.294438
5.545901	472.928936	7.299443
5.966317	467.626035	7.304448
5.884823	468.300486	7.309453
6.145081	473.669151	7.314458
5.950456	464.125634	7.319462
5.377123	465.112218	7.324467
6.027458	481.258639	7.329472
5.595573	463.147464	7.334477
5.684328	467.118690	7.339482
5.837394	473.416553	7.344486
5.785025	480.166373	7.349491
5.917326	474.437828	7.354496
5.968384	484.844220	7.359501
5.943628	469.901191	7.364506
6.183815	470.666620	7.369510
5.704326	477.035867	7.374515
5.806597	467.564732	7.379520
5.994815	465.370087	7.384525
6.288555	460.779208	7.389530
5.772191	474.894910	7.394534
5.912020	468.954294	7.399539
6.104870	463.897954	7.404544
5.749122	474.962811	7.409549
5.875882	471.235338	7.414554
5.775763	464.954944	7.419558
6.037268	467.795732	7.424563
6.026110	466.463535	7.429568
5.680942	465.814579	7.434573
5.909987	471.791190	7.439578
5.982776	474.690888	7.444582
5.993614	469.771468	7.449587
5.978885	459.301442	7.454592
5.986400	474.605505	7.459597
5.764791	465.976057	7.464602
5.905492	468.305842	7.469606
5.823811	473.739694	7.474611
5.992546	474.204487	7.479616
5.795344	472.244207	7.484621
5.886953	469.013260	7.489626
6.050624	462.122397	7.494630
5.518835	455.481523	7.499635
5.833429	475.252599	7.504640
5.774795	471.989653	7.509645
5.792364	474.297166	7.514650
6.253502	471.089701	7.519654
5.841277	470.195418	7.524659
6.012558	467.921194	7.529664
5.818286	448.730145	7.534669
5.591896	460.775369	7.539674
5.810054	448.710763	7.544678
5.512668	467.598570	7.549683
5.861368	455.840221	7.554688
6.224198	465.521850	7.559693
6.363996	464.264547	7.564698
6.166771	455.621703	7.569702
5.783538	443.897005	7.574707
5.760014	439.238201	7.579712
5.749603	439.173217	7.584717
5.983001	441.111207	7.589722
6.231174	433.455226	7.594726
6.063269	439.225033	7.599731
5.921650	435.707167	7.604736
5.684303	437.973929	7.609741
5.321500	432.708719	7.614746
5.609188	436.326431	7.619750
5.544568	445.490300	7.624755
5.757026	461.887825	7.629760
5.750958	468.032626	7.634765
5.847237	470.677855	7.639770
6.313141	474.798573	7.644774
5.976780	478.711109	7.649779
6.079294	464.554062	7.654784
6.118262	446.271670	7.659789
5.786443	447.461036	7.664794
5.771396	435.234804	7.669798
5.749810	444.906546	7.674803
5.439131	441.567363	7.679808
5.591717	465.860362	7.684813
5.826508	468.085017	7.689818
6.034321	470.736281	7.694822
5.998422	465.642171	7.699827
5.812066	469.630644	7.704832
5.752749	473.317054	7.709837
5.613410	466.184831	7.714842
5.528464	465.694822	7.719846
5.642041	476.025369	7.724851
5.912848	463.492806	7.729856
5.917678	472.630910	7.734861
6.135237	479.702237	7.739866
5.865794	470.321137	7.744870
5.764558	475.805873	7.749875
6.307373	476.911478	7.754880
6.018411	473.123168	7.759885
5.833522	474.569425	7.764890
6.080717	469.352665	7.769894
6.090243	470.257531	7.774899
6.296985	463.819583	7.779904
6.065052	445.890457	7.784909
5.785808	434.572013	7.789914
6.017115	438.240084	7.794918
5.611626	438.651881	7.799923
5.978983	430.761926	7.804928
5.541152	439.567092	7.809933
5.438147	436.859815	7.814938
5.855342	452.745806	7.819942
6.064427	467.379629	7.824947
5.870581	466.567843	7.829952
6.012456	466.320436	7.834957
5.811268	463.363600	7.839962
5.570019	448.517436	7.844966
5.867499	471.515613	7.849971
6.257987	468.231033	7.854976
6.023317	465.799450	7.859981
5.652428	451.040806	7.864986
6.060298	448.918190	7.869990
6.021720	454.918598	7.874995
5.951867	443.071279	7.880000
6.069457	444.603200	7.885005
5.591985	441.842277	7.890010
6.114288	438.851028	7.895014
5.931102	437.557423	7.900019
5.731757	438.363717	7.905024
5.551796	445.455140	7.910029
5.596053	440.263935	7.915034
5.960758	432.074502	7.920038
5.673483	453.068898	7.925043
5.955522	454.855505	7.930048
5.951795	455.056479	7.935053
6.200270	461.651310	7.940058
6.277408	443.093975	7.945062
5.848137	439.727133	7.950067
5.750579	429.407158	7.955072
5.739516	447.437365	7.960077
6.166993	443.268441	7.965082
6.326322	434.801095	7.970086
5.988879	442.112991	7.975091
5.834845	425.908249	7.980096
5.896540	435.226550	7.985101
5.762813	438.777263	7.990106
6.085962	435.834020	7.995110
5.417085	442.804583	8.000115
5.569036	434.847168	8.005133
5.382268	449.106693	8.010150
5.383951	444.316965	8.015168
5.830065	442.962893	8.020186
5.972748	469.812562	8.025203
6.102501	467.451836	8.030221
5.369958	472.670132	8.035238
5.703456	478.322865	8.040256
6.156969	472.936131	8.045274
5.766550	466.598244	8.050291
5.975218	463.319452	8.055309
6.001648	471.271271	8.060326
5.988979	474.672146	8.065344
6.266902	465.975762	8.070362
6.020138	474.493879	8.075379
6.127540	460.708053	8.080397
6.019815	459.979445	8.085414
5.880842	448.388220	8.090432
6.115122	430.225093	8.095450
5.660839	437.403661	8.100467
5.999003	450.023818	8.105485
6.074366	458.308023	8.110502
5.798277	465.968270	8.115520
6.238504	463.806481	8.120538
6.090225	452.281442	8.125555
6.171820	445.541812	8.130573
5.657386	447.375751	8.135590
5.531544	446.507943	8.140608
6.193636	451.221416	8.145626
5.883119	473.087998	8.150643
6.128246	456.990822	8.155661
6.545970	465.643661	8.160678
6.255980	455.610233	8.165696
6.194305	431.357055	8.170714
6.107796	441.063471	8.175731
5.773183	439.637376	8.180749
6.077874	429.772959	8.185766
5.808042	429.547319	8.190784
6.175950	434.735687	8.195802
6.220937	435.302725	8.200819
6.274682	430.093462	8.205837
6.067600	435.101710	8.210854
6.112164	437.106111	8.215872
6.266089	429.060715	8.220890
5.954123	437.333833	8.225907
5.885341	433.737096	8.230925
5.754444	422.827383	8.235942
5.877360	437.684501	8.240960
6.348622	454.523794	8.245978
6.076867	460.878775	8.250995
6.169709	457.351858	8.256013
6.174239	461.805374	8.261030
6.084677	453.969359	8.266048
6.169686	461.514136	8.271066
6.337842	467.150890	8.276083
6.122489	455.028597	8.281101
6.285004	439.070262	8.286118
5.934436	445.710349	8.291136
6.186225	442.642992	8.296154
5.892471	460.162334	8.301171
6.060477	468.896590	8.306189
6.389207	457.377251	8.311206
6.270164	473.636895	8.316224
6.219599	472.898939	8.321242
6.088911	473.632578	8.326259
6.187112	465.174709	8.331277
6.252648	470.966385	8.336294
5.980564	478.139267	8.341312
6.321596	474.134811	8.346330
6.555765	474.321645	8.351347
6.204199	465.249269	8.356365
6.219088	465.488970	8.361382
6.308105	472.700876	8.366400
6.296996	461.139682	8.371418
6.029286	458.017353	8.376435
6.376961	456.704148	8.381453
6.657661	449.064179	8.386470
6.222447	448.080897	8.391488
6.430582	444.653902	8.396506
6.442978	439.261745	8.401523
6.211606	446.785683	8.406541
6.287543	442.719355	8.411558
6.145622	440.856582	8.416576
6.237520	440.832921	8.421594
6.147680	442.829224	8.426611
6.312103	431.316096	8.431629
6.168982	444.348585	8.436646
6.139376	465.915935	8.441664
6.426357	462.634240	8.446682
6.684421	461.701219	8.451699
6.353591	449.277707	8.456717
6.402609	440.227417	8.461734
6.008898	438.079354	8.466752
6.314033	450.986800	8.471770
6.471807	463.104312	8.476787
6.332585	464.009010	8.481805
6.435886	455.480436	8.486822
6.066058	467.380774	8.491840
6.269047	460.108979	8.496858
6.560159	461.093418	8.501875
6.270069	469.551875	8.506893
6.353765	472.547439	8.511910
6.305907	471.054961	8.516928
6.440988	454.882194	8.521946
6.419086	470.518135	8.526963
6.193332	461.556143	8.531981
6.526687	462.005858	8.536998
6.286037	466.683121	8.542016
6.340711	462.458525	8.547034
6.303672	460.682333	8.552051
6.312415	468.001577	8.557069
6.389335	461.806692	8.562087
6.215888	466.565644	8.567104
6.470015	466.813438	8.572122
6.555178	470.616561	8.577139
6.223976	476.460517	8.582157
6.459204	454.469466	8.587175
6.338153	461.014557	8.592192
6.200847	467.628562	8.597210
6.223597	461.857797	8.602227
6.253956	477.570327	8.607245
6.593414	473.079914	8.612263
6.366285	485.498106	8.617280
6.780116	489.684034	8.622298
6.728033	492.999123	8.627315
6.481033	495.653555	8.632333
6.749475	468.312443	8.637351
6.348461	471.805242	8.642368
6.074811	472.579432	8.647386
6.540602	483.515392	8.652403
6.664978	495.203893	8.657421
6.641453	499.424802	8.662439
6.623908	495.700613	8.667456
6.662381	496.568568	8.672474
6.881184	495.000238	8.677491
6.615669	491.738494	8.682509
6.572884	479.530787	8.687527
6.491660	474.372054	8.692544
6.563437	487.613111	8.697562
6.903481	484.787505	8.702579
6.480881	496.905106	8.707597
6.652230	474.898209	8.712615
6.562557	471.697550	8.717632
6.718887	478.347566	8.722650
5.981143	487.454789	8.727667
6.378993	497.992033	8.732685
6.755073	500.529233	8.737703
6.659846	505.742103	8.742720
6.697967	490.397652	8.747738
6.769201	490.904952	8.752755
6.575199	496.507096	8.757773
6.962185	497.032085	8.762791
6.733134	493.861834	8.767808
6.913259	501.777446	8.772826
6.826791	499.620522	8.777843
6.669369	500.033747	8.782861
6.829513	501.064629	8.787879
6.825759	500.685788	8.792896
6.392711	491.317281	8.797914
6.626771	492.945072	8.802931
6.545081	497.421899	8.807949
6.743517	494.020901	8.812967
6.843179	491.164757	8.817984
6.674515	507.494927	8.823002
6.989275	490.670806	8.828019
6.785565	497.106762	8.833037
6.839218	499.214372	8.838055
6.617369	487.204225	8.843072
6.641865	493.619886	8.848090
7.058493	501.383250	8.853107
6.716603	501.889642	8.858125
6.793093	487.256322	8.863143
6.828358	506.699771	8.868160
6.602616	506.169465	8.873178
6.910687	494.058459	8.878195
6.634398	505.048377	8.883213
6.877716	495.839989	8.888231
6.648472	492.642118	8.893248
6.528194	503.596512	8.898266
7.216734	490.569565	8.903283
6.864979	496.294411	8.908301
6.900254	491.799842	8.913319
6.730532	497.293664	8.918336
6.424003	496.531582	8.923354
6.999530	498.447068	8.928371
6.449458	509.940012	8.933389
6.936211	493.741857	8.938407
6.957781	487.687282	8.943424
6.835753	501.772314	8.948442
7.390544	493.324687	8.953459
6.907435	499.202119	8.958477
6.846374	498.259344	8.963495
6.875015	486.912087	8.968512
7.036115	501.167903	8.973530
7.181348	491.780884	8.978547
6.998598	496.919061	8.983565
7.128054	489.906301	8.988583
6.970026	500.487483	8.993600
6.855489	497.002798	8.998618
6.893864	495.147126	9.003635
6.930729	506.743525	9.008653
6.893021	500.239191	9.013671
6.921374	497.461449	9.018688
6.871959	503.272527	9.023706
6.987995	488.207366	9.028723
6.772873	503.959997	9.033741
6.766327	498.402481	9.038759
6.804134	501.076371	9.043776
6.845971	494.613705	9.048794
7.036970	497.855168	9.053811
6.706419	506.538396	9.058829
7.046437	511.406861	9.063847
7.186254	522.506831	9.068864
7.172872	531.931886	9.073882
6.831384	521.781360	9.078899
7.099038	533.269872	9.083917
7.004779	531.434145	9.088935
6.919958	525.027921	9.093952
7.137397	527.919030	9.098970
7.328965	524.716855	9.103987
7.079156	523.971377	9.109005
7.094936	536.097847	9.114023
7.000020	546.420750	9.119040
7.002988	532.190303	9.124058
7.260417	522.970709	9.129075
6.817258	541.359344	9.134093
7.226870	537.585811	9.139111
7.063763	526.199261	9.144128
6.992022	532.984509	9.149146
7.359442	528.870188	9.154163
7.056406	523.611311	9.159181
7.186459	518.565159	9.164199
6.911463	526.002170	9.169216
6.839005	536.586064	9.174234
7.061607	526.231613	9.179251
7.179581	527.685718	9.184269
6.939341	526.795775	9.189287
7.120964	527.020225	9.194304
7.019693	542.187269	9.199322
7.054986	526.502275	9.204339
7.103972	530.737485	9.209357
7.184942	535.791649	9.214375
7.165145	535.957375	9.219392
7.235026	545.373402	9.224410
7.434010	553.261323	9.229427
7.410313	548.015123	9.234445
7.534300	536.212597	9.239463
7.096292	533.398159	9.244480
6.777314	539.218174	9.249498
7.175132	546.137895	9.254515
7.372645	547.644002	9.259533
7.390193	563.630237	9.264551
7.649804	563.864629	9.269568
7.256451	546.019017	9.274586
7.290553	532.935353	9.279603
7.336722	539.843707	9.284621
7.046546	540.776504	9.289639
7.502697	542.560966	9.294656
7.412299	561.029589	9.299674
7.245900	563.401772	9.304691
7.577274	560.158675	9.309709
7.597971	551.599121	9.314727
7.375028	541.882737	9.319744
6.992481	537.009852	9.324762
7.507330	544.586766	9.329779
7.396619	549.976682	9.334797
7.500611	547.099442	9.339815
7.425088	550.366164	9.344832
7.275870	541.058968	9.349850
7.233853	548.737846	9.354867
7.452876	563.264012	9.359885
7.222171	563.235504	9.364903
7.792555	558.595314	9.369920
7.516818	567.631354	9.374938
7.551387	558.465197	9.379955
7.358297	538.603736	9.384973
7.204102	556.931845	9.389991
7.590875	566.394514	9.395008
7.644106	562.283689	9.400026
7.601935	562.541677	9.405043
7.715724	548.329606	9.410061
7.197231	542.432254	9.415079
7.530112	529.091683	9.420096
7.383219	543.212942	9.425114
7.345536	552.777234	9.430131
7.799477	561.421289	9.435149
7.375636	566.325565	9.440167
7.622630	559.840975	9.445184
7.743782	565.888895	9.450202
7.716944	551.207544	9.455219
7.854687	543.442068	9.460237
7.413222	538.528042	9.465255
7.757081	535.825492	9.470272
7.316179	536.280545	9.475290
7.351781	527.622694	9.480307
7.295411	528.822106	9.485325
7.331748	558.920333	9.490343
8.039857	561.379255	9.495360
7.722404	557.070390	9.500378
7.505308	557.474485	9.505395
7.709558	551.642892	9.510413
7.467906	561.822371	9.515431
7.763636	547.838253	9.520448
7.609760	554.997836	9.525466
7.560174	561.865245	9.530483
7.575665	570.123978	9.535501
7.478193	562.789605	9.540519
7.934887	557.853110	9.545536
7.480347	567.326881	9.550554
7.979145	561.112427	9.555571
8.002398	562.074910	9.560589
7.572273	560.073861	9.565607
7.659822	546.706803	9.570624
7.987289	558.155830	9.575642
7.583295	554.039577	9.580659
7.714593	548.703111	9.585677
7.527057	542.432825	9.590695
7.667592	553.561729	9.595712
7.539708	572.370841	9.600730
7.701026	560.462344	9.605747
7.821104	553.147723	9.610765
7.782239	578.696360	9.615783
7.664039	570.394149	9.620800
7.435986	559.969885	9.625818
7.389333	568.930773	9.630835
7.988894	565.535603	9.635853
7.489948	559.841172	9.640871
7.778726	563.407661	9.645888
7.825101	568.250471	9.650906
7.751008	564.087276	9.655923
7.515924	565.431554	9.660941
7.216369	577.862674	9.665959
7.827087	572.551974	9.670976
7.538729	581.094440	9.675994
7.587655	597.063125	9.681011
8.301481	596.442891	9.686029
8.037418	600.069650	9.691047
8.161767	599.042993	9.696064
7.819933	572.668119	9.701082
7.797164	572.393678	9.706099
7.553200	570.286879	9.711117
8.045811	585.885837	9.716135
8.159767	600.764569	9.721152
8.239847	590.580841	9.726170
7.942661	577.253914	9.731187
7.785936	562.575318	9.736205
7.464155	573.437004	9.741223
7.863533	584.693299	9.746240
7.703545	591.863454	9.751258
8.033913	597.482209	9.756275
8.104437	600.182986	9.761293
8.078204	604.998051	9.766311
8.198351	589.604815	9.771328
8.274093	592.054387	9.776346
7.828088	582.217882	9.781363
7.904849	567.174583	9.786381
7.668322	576.605347	9.791399
7.821592	593.954828	9.796416
8.058928	596.523041	9.801434
7.938263	605.191321	9.806451
7.981072	602.997668	9.811469
8.074985	607.259128	9.816487
8.029096	601.349389	9.821504
8.143307	612.492821	9.826522
8.067889	606.828363	9.831539
8.238459	605.142428	9.836557
8.214129	613.612448	9.841575
7.965940	611.687703	9.846592
8.211957	605.887271	9.851610
8.270654	599.395796	9.856627
8.261129	593.567729	9.861645
7.940056	601.600560	9.866663
7.918798	599.037453	9.871680
8.226779	600.142612	9.876698
7.928351	603.209319	9.881715
8.324254	602.190138	9.886733
8.390153	605.998250	9.891751
8.330642	592.020346	9.896768
8.176049	606.006840	9.901786
7.924860	600.971015	9.906803
8.216056	602.629526	9.911821
8.040788	613.972931	9.916839
7.770123	593.951910	9.921856
8.024909	602.614334	9.926874
7.955345	609.770047	9.931891
8.384504	599.189424	9.936909
7.785831	601.225945	9.941927
8.366002	597.386621	9.946944
8.168439	599.929773	9.951962
8.057155	602.040052	9.956979
8.310622	596.274900	9.961997
7.929474	615.273919	9.967015
8.128022	601.975854	9.972032
8.221288	602.592684	9.977050
8.041161	613.642857	9.982067
8.270127	621.557053	9.987085
8.474618	637.051835	9.992103
8.529866	630.524113	9.997120
8.482824	615.833836	10.002138
8.145803	608.958136	10.007155
8.231852	599.619505	10.012173
8.025561	617.619354	10.017191
8.197415	625.948618	10.022208
8.456318	636.985103	10.027226
8.284584	632.288331	10.032243
8.426275	627.951101	10.037261
8.637900	641.726057	10.042279
8.566085	625.021469	10.047296
8.377742	636.398934	10.052314
8.076613	634.946031	10.057331
8.552422	640.281370	10.062349
8.427182	635.309447	10.067367
8.552071	625.490756	10.072384
8.219022	633.328378	10.077402
8.223990	635.682193	10.082419
8.460015	630.030617	10.087437
8.698473	636.960477	10.092455
8.721845	637.583938	10.097472
8.410671	628.703569	10.102490
8.424708	646.342698	10.107507
8.857605	633.767342	10.112525
8.725361	628.882881	10.117543
8.683916	611.293838	10.122560
8.623089	603.296731	10.127578
8.039192	612.448078	10.132595
8.503285	608.103433	10.137613
8.509687	612.271209	10.142631
8.519806	626.277147	10.147648
8.560433	628.187853	10.152666
8.346109	637.146475	10.157683
8.390208	635.071773	10.162701
8.437323	642.302098	10.167719
8.843208	640.034664	10.172736
8.643244	639.994975	10.177754
8.617545	642.246006	10.182771
8.489380	640.270425	10.187789
8.491475	646.500126	10.192807
8.464525	631.987580	10.197824
8.551633	637.150387	10.202842
8.378613	643.970920	10.207859
8.440629	627.667554	10.212877
8.224477	635.090072	10.217895
8.348918	642.057767	10.222912
8.646076	631.972660	10.227930
8.235166	645.030775	10.232947
8.616995	625.945085	10.237965
8.703992	648.181966	10.242983
8.630207	663.486094	10.248000
8.855773	658.053517	10.253018
8.539716	658.007722	10.258035
9.035854	658.218873	10.263053
8.531422	657.323968	10.268071
8.495530	658.434294	10.273088
8.979483	661.158674	10.278106
8.999547	674.608889	10.283123
8.722882	640.712898	10.288141
8.515787	650.679876	10.293159
8.388107	657.539666	10.298176
8.774485	666.966938	10.303194
8.647934	674.506729	10.308211
8.974804	660.070601	10.313229
9.172945	658.873411	10.318247
8.878506	670.885537	10.323264
8.790628	664.164566	10.328282
8.787626	658.340022	10.333299
8.664496	663.408177	10.338317
8.692534	667.965622	10.343335
8.651766	660.355841	10.348352
8.776767	678.914379	10.353370
8.751942	674.419650	10.358387
8.660559	667.267748	10.363405
8.880698	684.091618	10.368423
8.496780	679.536075	10.373440
8.881507	665.788768	10.378458
8.920534	678.735756	10.383475
9.016106	673.786375	10.388493
8.962019	671.524981	10.393511
8.810143	670.548098	10.398528
8.724873	672.475087	10.403546
8.535795	672.048340	10.408563
8.749578	665.012709	10.413581
9.027093	681.181357	10.418599
9.041501	680.077409	10.423616
9.093713	660.765885	10.428634
8.962718	673.763893	10.433651
8.959066	666.851380	10.438669
8.960946	664.953696	10.443687
8.924937	672.459729	10.448704
9.226327	682.916111	10.453722
8.825967	679.987277	10.458739
9.065785	690.119652	10.463757
9.362854	685.593081	10.468775
8.850701	677.736745	10.473792
9.060156	685.391553	10.478810
9.226485	681.202471	10.483827
8.909123	674.041363	10.488845
9.391253	673.789172	10.493863
9.007383	685.905539	10.498880
9.124504	674.937736	10.503898
8.622152	682.694129	10.508915
8.924887	690.631990	10.513933
9.226195	690.049023	10.518951
9.342677	695.042461	10.523968
9.447565	705.163096	10.528986
9.287199	697.433422	10.534003
9.377085	684.992449	10.539021
9.024408	670.736999	10.544039
8.794693	678.615824	10.549056
9.236162	691.488249	10.554074
8.909152	699.903927	10.559091
9.323728	698.823595	10.564109
9.556612	698.251837	10.569127
9.223847	704.700644	10.574144
9.303441	688.874628	10.579162
8.918215	684.862894	10.584179
9.424419	694.225213	10.589197
9.715532	687.241642	10.594215
9.115791	674.462464	10.599232
9.281584	669.331140	10.604250
9.214265	668.618478	10.609267
9.220774	687.615717	10.614285
9.353016	674.949193	10.619303
9.164312	690.380880	10.624320
9.498486	699.328116	10.629338
9.216465	690.610577	10.634355
9.417874	697.220469	10.639373
9.358081	694.354129	10.644391
9.206667	696.345879	10.649408
9.508095	686.492072	10.654426
9.322466	691.522246	10.659443
9.418819	707.238670	10.664461
9.560651	684.827671	10.669479
9.007875	702.477379	10.674496
9.376405	702.588480	10.679514
9.335192	698.044790	10.684531
9.443761	694.933249	10.689549
9.769057	686.871208	10.694567
9.216699	701.813995	10.699584
9.357434	690.473059	10.704602
9.442994	700.215955	10.709619
9.518071	698.252146	10.714637
9.630672	690.147020	10.719655
9.543275	694.817723	10.724672
9.712740	696.243260	10.729690
9.738264	695.200257	10.734707
9.417575	681.277930	10.739725
9.398811	672.384739	10.744743
9.512699	691.674611	10.749760
9.521021	689.105518	10.754778
9.162251	699.232605	10.759795
9.240454	690.298385	10.764813
9.607815	689.948353	10.769831
9.337866	697.864735	10.774848
9.461713	693.771432	10.779866
9.387959	698.982591	10.784883
9.376414	702.115666	10.789901
9.509436	694.486301	10.794919
9.291132	698.630911	10.799936
9.236967	695.849253	10.804954
9.558335	694.057204	10.809971
9.318643	708.439570	10.814989
9.310388	720.622313	10.820007
9.602201	726.292261	10.825024
9.904625	730.558858	10.830042
9.758029	729.236186	10.835059
9.561176	728.149433	10.840077
10.062882	725.032947	10.845095
9.709977	733.127985	10.850112
9.492631	721.467533	10.855130
9.729866	733.760083	10.860147
9.817604	723.935856	10.865165
10.102121	719.610425	10.870183
9.893493	717.545297	10.875200
9.739110	699.953659	10.880218
9.291518	689.963243	10.885235
9.560480	714.149190	10.890253
9.814263	718.115123	10.895271
9.579660	718.565708	10.900288
9.497647	725.444748	10.905306
9.686778	726.895773	10.910323
9.491514	728.186250	10.915341
9.834695	718.382991	10.920359
9.860778	722.713556	10.925376
10.082816	726.935967	10.930394
9.944541	727.517161	10.935411
9.874922	726.622038	10.940429
9.901977	734.902567	10.945447
9.808258	732.884380	10.950464
9.883040	732.961953	10.955482
9.998311	723.044612	10.960499
9.391543	729.523554	10.965517
10.152958	728.736034	10.970535
9.694367	739.555792	10.975552
9.686652	729.230211	10.980570
10.041741	726.583636	10.985587
10.023717	734.430262	10.990605
10.156177	729.408638	10.995623
9.617476	731.790511	11.000640
9.601672	728.617740	11.005658
9.811621	729.306024	11.010675
9.725549	745.683809	11.015693
10.240748	741.421512	11.020711
9.777333	756.360380	11.025728
10.101390	771.706824	11.030746
10.449611	762.721840	11.035763
9.839114	749.011681	11.040781
10.194516	747.006954	11.045799
9.863347	735.246622	11.050816
10.212974	743.428485	11.055834
9.797328	750.739270	11.060851
9.987926	760.015031	11.065869
10.162104	747.442875	11.070887
10.177457	757.186880	11.075904
10.206938	769.606390	11.080922
10.336400	770.563243	11.085939
9.987086	755.195462	11.090957
10.418552	751.174120	11.095975
10.057258	753.958683	11.100992
10.098366	742.701974	11.106010
10.192214	748.499016	11.111027
10.066617	752.676637	11.116045
10.323720	754.643694	11.121063
10.492677	751.577565	11.126080
10.398299	754.225911	11.131098
10.124287	733.371071	11.136115
9.910629	732.706403	11.141133
9.979302	734.226046	11.146151
9.895286	755.461619	11.151168
10.127797	761.039824	11.156186
10.534221	753.336713	11.161203
10.181230	773.363555	11.166221
10.291089	758.569374	11.171239
10.228281	758.037817	11.176256
10.040558	771.504643	11.181274
10.191605	767.186986	11.186291
10.264458	767.635280	11.191309
10.581679	751.397857	11.196327
10.383485	761.590459	11.201344
10.006657	776.429523	11.206362
10.413936	758.818511	11.211379
10.248664	770.960719	11.216397
10.494190	762.560116	11.221415
10.241910	767.625932	11.226432
10.477120	761.459089	11.231450
10.385073	764.720714	11.236467
10.445778	771.296814	11.241485
10.648899	757.612499	11.246503
10.753367	758.643153	11.251520
10.907839	762.372801	11.256538
10.772626	766.927337	11.261555
10.364912	770.032112	11.266573
10.459531	757.597087	11.271591
10.597779	762.306099	11.276608
10.592438	767.999483	11.281626
10.402426	761.169880	11.286643
10.296362	763.982333	11.291661
10.668574	766.971016	11.296679
10.456893	767.297366	11.301696
10.262010	767.689332	11.306714
10.312168	769.989547	11.311731
10.382090	774.241242	11.316749
10.385795	768.622398	11.321767
10.629131	778.052613	11.326784
10.176250	772.084497	11.331802
10.390786	760.403227	11.336819
10.151275	777.060585	11.341837
10.341237	779.326481	11.346855
10.632419	782.607540	11.351872
10.616420	802.057669	11.356890
10.768764	808.055755	11.361907
10.557965	802.259886	11.366925
10.490819	804.793329	11.371943
10.773829	809.612069	11.376960
10.706898	814.849595	11.381978
10.945325	804.128434	11.386995
10.888545	803.553171	11.392013
10.746474	787.400760	11.397031
10.853645	777.955302	11.402048
10.272812	779.102451	11.407066
10.633541	779.555034	11.412083
10.695052	790.809253	11.417101
10.637123	806.329957	11.422119
11.075391	789.453414	11.427136
10.529886	799.588988	11.432154
10.671780	798.613444	11.437171
10.787259	802.576175	11.442189
10.821771	794.613893	11.447207
10.960428	805.881060	11.452224
10.935115	799.094583	11.457242
10.965694	792.307730	11.462259
10.968819	807.181950	11.467277
10.625738	801.188691	11.472295
10.694678	799.272922	11.477312
10.811720	795.922899	11.482330
11.009966	800.630274	11.487347
10.851371	801.858113	11.492365
10.945244	791.669807	11.497383
11.046725	800.415836	11.502400
10.871222	809.878480	11.507418
11.058623	801.513835	11.512435
11.019520	796.642368	11.517453
10.798799	787.858749	11.522471
11.358488	795.932811	11.527488
10.790802	805.704210	11.532506
11.199635	789.091932	11.537523
11.043560	792.879203	11.542541
10.991235	802.619758	11.547559
11.004375	794.346106	11.552576
10.747457	804.204904	11.557594
10.911485	806.535314	11.562611
10.975063	800.623842	11.567629
10.674288	794.799447	11.572647
11.123741	799.092938	11.577664
10.872579	805.174137	11.582682
10.944854	795.813062	11.587699
10.806443	805.690950	11.592717
10.928671	797.035953	11.597735
10.905115	793.328627	11.602752
10.966633	818.130011	11.607770
11.169610	822.207102	11.612787
11.595471	833.221847	11.617805
10.887053	829.442090	11.622823
11.491739	830.898358	11.627840
11.028314	828.143862	11.632858
11.121242	818.590518	11.637875
11.231395	834.131791	11.642893
11.618140	824.672776	11.647911
10.963913	806.563432	11.652928
11.141409	821.021621	11.657946
11.287059	828.869293	11.662963
11.605895	834.906991	11.667981
11.389861	827.952351	11.672999
11.545660	796.979757	11.678016
11.218003	801.742154	11.683034
11.151246	795.234229	11.688051
11.348768	808.693615	11.693069
11.152491	814.067258	11.698087
11.628949	810.935541	11.703104
11.418144	805.148037	11.708122
11.368456	802.760428	11.713139
11.458646	802.139720	11.718157
11.489893	804.547574	11.723175
11.631437	801.712005	11.728192
11.125904	804.546785	11.733210
11.438300	795.940663	11.738227
11.503582	798.930772	11.743245
11.239586	810.741949	11.748263
11.342529	791.276335	11.753280
11.149150	810.918945	11.758298
11.357829	828.366405	11.763315
11.513559	827.002522	11.768333
11.364985	825.963187	11.773351
11.626151	835.971780	11.778368
11.382693	831.175993	11.783386
11.322426	835.566224	11.788403
11.217885	837.982941	11.793421
11.515457	848.648100	11.798439
11.425400	821.304592	11.803456
11.617846	825.072263	11.808474
11.768772	834.655061	11.813491
12.206206	839.300583	11.818509
11.818207	826.244206	11.823527
11.524459	830.025895	11.828544
11.695184	830.024142	11.833562
11.674882	824.895571	11.838579
11.895207	837.296393	11.843597
11.670127	820.284402	11.848615
11.667812	804.647950	11.853632
11.724409	810.271087	11.858650
11.506617	804.863406	11.863667
11.567338	810.618710	11.868685
11.519463	817.443143	11.873703
11.586885	822.772424	11.878720
11.701344	828.281892	11.883738
11.717820	814.474954	11.888755
11.957017	821.248899	11.893773
11.393891	825.863144	11.898791
11.364687	825.451008	11.903808
11.530518	823.932533	11.908826
11.731369	826.129129	11.913843
11.996464	825.559719	11.918861
11.677828	825.425094	11.923879
11.712648	827.203738	11.928896
11.871768	837.927785	11.933914
11.908028	827.158043	11.938931
11.906719	828.178332	11.943949
11.587512	833.374399	11.948967
12.052302	830.062653	11.953984
12.105980	824.479125	11.959002
12.077393	833.020429	11.964019
11.829186	829.518100	11.969037
11.807830	829.015806	11.974055
11.821573	830.674728	11.979072
11.691712	836.049703	11.984090
11.680005	827.147187	11.989107
12.054969	832.030645	11.994125
11.962265	837.403023	11.999143
11.950392	818.865430	12.004160
11.861914	823.896716	12.009178
11.770878	827.859040	12.014195
12.463903	842.514288	12.019213
12.044493	835.584396	12.024231
12.280995	834.799772	12.029248
11.992456	838.343639	12.034266
11.889026	830.941730	12.039283
12.217164	828.947403	12.044301
11.753002	834.963929	12.049319
12.321884	851.279945	12.054336
12.101320	840.501561	12.059354
11.770423	841.241535	12.064371
12.193538	846.212102	12.069389
12.247838	861.057744	12.074407
12.281418	852.914615	12.079424
12.209258	859.535146	12.084442
12.196191	857.477340	12.089459
12.352181	848.224521	12.094477
12.177665	855.392575	12.099495
12.023551	850.786310	12.104512
12.045559	855.230655	12.109530
12.020175	864.819383	12.114547
12.320474	862.902670	12.119565
11.953545	860.662833	12.124583
11.990248	870.114458	12.129600
12.136215	864.405449	12.134618
12.015560	870.344164	12.139635
11.918218	874.132574	12.144653
12.007271	871.088778	12.149671
11.927601	867.079642	12.154688
12.493015	875.096708	12.159706
12.256007	891.305729	12.164723
12.450870	878.335337	12.169741
12.532945	875.019909	12.174759
12.461829	875.274714	12.179776
12.241099	873.997246	12.184794
12.335855	884.322293	12.189811
12.623985	878.835804	12.194829
12.410195	879.322416	12.199847
12.525126	863.225174	12.204864
12.222645	865.884212	12.209882
12.359611	879.872962	12.214899
12.800873	882.708847	12.219917
12.680122	880.978028	12.224935
12.815581	857.858217	12.229952
12.781697	858.954547	12.234970
12.542949	862.490881	12.239987
12.529944	860.180552	12.245005
12.087850	865.451159	12.250023
12.481198	850.934589	12.255040
12.598346	855.879553	12.260058
12.297602	857.339608	12.265075
12.582590	872.083273	12.270093
12.301620	887.442036	12.275111
12.670515	894.824583	12.280128
12.627662	892.924225	12.285146
12.530157	901.106355	12.290163
12.777018	889.729824	12.295181
12.742565	896.313338	12.300199
12.562071	885.426352	12.305216
12.784447	889.140381	12.310234
12.410167	896.122311	12.315251
12.863909	895.678192	12.320269
12.750140	894.372912	12.325287
12.471549	889.220872	12.330304
12.841128	886.797031	12.335322
12.679062	900.776170	12.340339
12.558590	881.876792	12.345357
12.559302	894.985777	12.350375
12.671633	896.064541	12.355392
12.775469	886.570462	12.360410
12.042186	906.901123	12.365427
12.545318	903.071111	12.370445
12.621325	908.311421	12.375463
12.931910	921.909675	12.380480
13.055500	918.689130	12.385498
12.818470	932.857820	12.390515
13.136392	923.857280	12.395533
13.213070	926.009462	12.400551
12.757360	908.209946	12.405568
12.900398	911.245484	12.410586
12.812172	924.028210	12.415603
13.166514	928.423266	12.420621
13.090625	934.473682	12.425639
13.147679	927.285321	12.430656
12.965248	899.874965	12.435674
12.853533	903.749502	12.440691
13.097512	892.435049	12.445709
12.910741	903.656377	12.450727
13.129214	919.026912	12.455744
13.087079	910.616788	12.460762
12.962270	904.667325	12.465779
13.125725	917.755734	12.470797
13.416437	923.350360	12.475815
13.056100	904.260319	12.480832
12.893342	893.771307	12.485850
12.772510	904.443452	12.490867
13.051131	916.873379	12.495885
13.143831	920.744351	12.500903
12.775021	920.075988	12.505920
13.079961	910.172451	12.510938
12.984590	923.413951	12.515955
13.269700	926.650679	12.520973
13.399122	923.205194	12.525991
13.286308	927.309995	12.531008
13.750255	918.744005	12.536026
13.249186	916.082115	12.541043
13.166299	919.497743	12.546061
13.417838	920.972031	12.551079
13.086504	924.762120	12.556096
13.692548	914.124399	12.561114
13.346132	916.363913	12.566131
13.224419	924.861613	12.571149
13.174046	918.248092	12.576167
13.000613	930.949842	12.581184
13.373148	913.522021	12.586202
13.161445	921.532418	12.591219
13.176345	928.135343	12.596237
13.286957	927.991681	12.601255
13.424019	925.569453	12.606272
13.664634	926.052715	12.611290
12.744943	921.651077	12.616307
12.965744	920.415385	12.621325
12.853197	923.636935	12.626343
12.553566	939.199780	12.631360
12.948391	942.541883	12.636378
12.915137	945.872654	12.641395
13.216391	951.762150	12.646413
14.030065	965.595655	12.651431
13.738221	962.977416	12.656448
13.859521	961.951338	12.661466
13.780914	955.214439	12.666483
13.795418	941.205978	12.671501
13.720593	945.483903	12.676519
13.646874	947.767614	12.681536
14.037435	936.363072	12.686554
13.820962	953.991245	12.691571
13.554979	947.435582	12.696589
13.838569	940.058526	12.701607
13.562070	941.941277	12.706624
14.064309	943.616714	12.711642
13.982387	940.306526	12.716659
13.723158	937.234164	12.721677
13.914691	938.242471	12.726695
13.462907	943.837384	12.731712
14.068001	941.339582	12.736730
13.778837	941.360194	12.741747
13.929962	940.277721	12.746765
13.658842	936.402449	12.751783
13.927833	948.116110	12.756800
13.774077	935.946749	12.761818
13.597237	943.124280	12.766835
13.887078	943.182258	12.771853
13.824394	936.561120	12.776871
13.861441	941.185058	12.781888
13.995790	936.654896	12.786906
13.934241	936.767103	12.791923
13.729876	934.294523	12.796941
13.720222	944.610392	12.801959
13.511627	944.242069	12.806976
13.692079	935.565465	12.811994
13.808744	948.579265	12.817011
13.978393	949.732011	12.822029
13.871352	940.304926	12.827047
13.935526	939.073761	12.832064
14.030166	937.933213	12.837082
14.132416	938.019927	12.842099
13.832773	938.766255	12.847117
14.011454	939.791644	12.852135
13.676455	942.753555	12.857152
13.648846	941.358947	12.862170
14.112326	959.975354	12.867187
14.109791	961.257520	12.872205
14.538806	968.780240	12.877223
14.169486	960.747425	12.882240
14.069998	948.009344	12.887258
14.111461	942.434877	12.892275
13.882225	953.085213	12.897293
14.338177	972.423518	12.902311
14.296885	971.665210	12.907328
14.285881	966.004835	12.912346
14.211610	963.860787	12.917363
14.323992	960.080277	12.922381
14.373644	953.102538	12.927399
14.384705	947.341100	12.932416
14.313996	935.813114	12.937434
13.737928	948.063396	12.942451
13.787482	955.268864	12.947469
14.470765	963.008080	12.952487
14.402294	978.392338	12.957504
14.360978	965.868605	12.962522
14.535444	962.914595	12.967539
14.263410	971.745177	12.972557
14.371983	971.821301	12.977575
14.182358	973.330511	12.982592
14.023952	966.293070	12.987610
14.507241	965.423276	12.992627
14.572178	974.679093	12.997645
14.806148	963.064918	13.002663
14.526711	973.064036	13.007680
14.679278	974.423015	13.012698
14.470506	962.838606	13.017715
14.497103	976.759182	13.022733
14.514935	970.147948	13.027751
14.401134	974.949160	13.032768
14.466872	970.232428	13.037786
14.480722	982.255256	13.042803
14.379273	976.474808	13.047821
14.701250	977.762198	13.052839
14.463034	966.135121	13.057856
14.643982	973.454392	13.062874
14.922523	972.933140	13.067891
14.649161	969.740786	13.072909
14.910039	971.580301	13.077927
14.660526	976.750335	13.082944
14.929260	966.207583	13.087962
14.902589	969.292237	13.092979
14.856114	974.473297	13.097997
15.118670	974.090587	13.103015
14.405899	970.504885	13.108032
14.618219	969.363488	13.113050
14.901121	962.394042	13.118067
14.619297	969.471632	13.123085
14.872786	964.325423	13.128103
15.097906	977.603461	13.133120
14.772586	959.198288	13.138138
15.073454	966.952186	13.143155
14.841894	973.307524	13.148173
14.814540	961.319482	13.153191
14.980380	967.767486	13.158208
15.109889	961.322316	13.163226
14.726818	958.332805	13.168243
14.564705	965.044708	13.173261
14.906325	963.682472	13.178279
14.748324	970.861823	13.183296
14.553049	963.388232	13.188314
14.985795	973.073436	13.193331
14.982334	968.582669	13.198349
14.854644	959.660273	13.203367
15.105537	968.017697	13.208384
14.993479	969.538986	13.213402
15.203277	969.829346	13.218419
14.681565	974.196478	13.223437
14.909188	965.658690	13.228455
15.119049	968.883851	13.233472
14.833525	963.066909	13.238490
14.922848	955.628560	13.243507
14.693050	965.854074	13.248525
14.907942	982.027582	13.253543
15.226001	989.732103	13.258560
15.135897	990.684315	13.263578
15.578991	989.797642	13.268595
14.944181	1000.138819	13.273613
14.883350	987.359382	13.278631
14.898792	986.444086	13.283648
14.945265	998.317566	13.288666
15.355202	989.136655	13.293683
15.161535	991.027570	13.298701
15.327570	994.628417	13.303719
15.474904	998.494810	13.308736
15.596787	990.845096	13.313754
15.643705	993.592652	13.318771
15.476584	996.567965	13.323789
15.252248	987.193299	13.328807
15.124240	999.644335	13.333824
15.223114	999.903329	13.338842
15.347284	983.685951	13.343859
15.021349	995.078939	13.348877
15.118574	991.457197	13.353895
15.320678	998.460342	13.358912
15.252778	995.115941	13.363930
15.457922	995.440922	13.368947
15.357690	1007.113199	13.373965
15.706296	1022.282247	13.378983
15.634476	1009.246483	13.384000
15.566325	1008.037278	13.389018
15.586768	995.715581	13.394035
15.236308	1008.065120	13.399053
15.699742	1005.226313	13.404071
15.911786	1009.769592	13.409088
15.593397	1009.888225	13.414106
15.669442	996.253040	13.419123
15.599371	1001.141899	13.424141
15.857042	1006.886085	13.429159
15.795905	1004.936480	13.434176
16.011918	992.621142	13.439194
15.766266	991.620077	13.444211
15.543076	997.731860	13.449229
15.618154	988.912038	13.454247
15.654789	992.088087	13.459264
15.487167	998.215586	13.464282
15.450770	1001.363358	13.469299
15.644718	1009.880386	13.474317
15.736689	1026.659288	13.479335
15.879026	1016.567138	13.484352
15.960011	1019.530290	13.489370
15.898514	1029.928885	13.494387
15.568824	1031.699690	13.499405
15.612298	1023.397973	13.504423
15.754798	1026.774706	13.509440
16.070499	1026.090942	13.514458
16.111393	1015.956806	13.519475
15.856234	1018.992235	13.524493
15.935193	1014.659162	13.529511
16.120266	1016.847076	13.534528
16.220961	1018.016634	13.539546
16.347087	1014.784924	13.544563
15.962467	1019.082080	13.549581
15.936790	1019.384488	13.554599
15.927915	1021.183069	13.559616
15.884735	1018.500505	13.564634
16.060952	1018.156861	13.569651
15.904842	1025.181720	13.574669
16.105727	1013.779336	13.579687
16.235157	1017.660697	13.584704
15.925381	1024.026522	13.589722
16.180551	1013.784254	13.594739
15.888470	1014.071738	13.599757
15.725624	1019.500743	13.604775
16.056461	1017.574537	13.609792
16.012845	1021.294273	13.614810
16.268564	1020.905902	13.619827
16.243109	1024.858916	13.624845
16.283828	1031.258244	13.629863
16.356162	1033.772808	13.634880
15.873594	1029.861207	13.639898
16.165791	1038.315861	13.644915
16.052960	1045.633526	13.649933
16.471313	1035.985824	13.654951
16.304495	1044.561700	13.659968
16.320778	1040.456755	13.664986
16.853336	1035.121813	13.670003
16.423722	1050.015425	13.675021
16.481356	1039.716429	13.680039
16.893399	1033.569854	13.685056
16.400310	1039.377004	13.690074
16.524964	1051.931186	13.695091
16.551512	1052.688565	13.700109
16.629838	1037.513174	13.705127
16.739580	1031.354951	13.710144
16.443027	1028.687980	13.715162
16.486042	1008.801557	13.720179
16.323290	1020.306254	13.725197
16.236723	1031.528929	13.730215
16.350742	1039.464009	13.735232
16.357457	1037.257561	13.740250
16.667333	1049.069741	13.745267
16.782834	1032.431868	13.750285
16.508146	1036.188907	13.755303
16.685971	1032.932215	13.760320
16.877936	1043.977103	13.765338
16.698042	1041.263691	13.770355
17.111119	1034.190826	13.775373
16.834018	1045.907811	13.780391
16.996733	1035.722335	13.785408
16.582107	1034.604432	13.790426
16.835825	1039.802233	13.795443
16.721215	1042.636913	13.800461
16.660809	1035.274047	13.805479
16.853004	1037.197644	13.810496
16.797131	1040.988985	13.815514
16.851755	1039.556275	13.820531
16.745479	1037.259758	13.825549
16.843373	1045.545477	13.830567
16.802111	1034.533918	13.835584
16.500805	1044.171896	13.840602
16.930043	1035.098379	13.845619
16.484475	1037.802053	13.850637
16.380365	1042.430945	13.855655
16.723463	1049.520934	13.860672
16.820622	1065.297520	13.865690
16.924910	1062.779031	13.870707
16.997955	1065.971713	13.875725
16.958378	1067.238556	13.880743
17.162144	1068.537025	13.885760
16.975297	1072.530891	13.890778
16.955948	1072.655611	13.895795
17.060742	1075.110989	13.900813
17.085746	1069.596076	13.905831
17.556505	1064.119984	13.910848
17.094419	1073.346928	13.915866
17.305028	1063.799275	13.920883
17.590748	1065.326187	13.925901
17.392836	1070.135226	13.930919
17.788778	1061.594369	13.935936
17.606912	1053.415391	13.940954
17.393918	1046.467825	13.945971
17.385768	1035.525288	13.950989
17.200360	1036.062716	13.956007
17.420974	1022.359925	13.961024
17.251214	1032.042091	13.966042
17.244520	1022.721974	13.971059
17.259823	1030.310040	13.976077
17.246875	1039.235815	13.981095
17.676789	1040.943093	13.986112
17.401468	1045.975805	13.991130
17.419764	1038.182780	13.996147
17.628308	1030.966777	14.001165
17.208566	1037.759271	14.006183
17.685165	1048.793439	14.011200
17.607162	1049.750445	14.016218
17.149004	1034.526628	14.021235
17.328445	1045.568273	14.026253
17.448088	1058.061094	14.031271
17.648714	1068.902832	14.036288
17.703556	1071.766002	14.041306
17.359675	1062.019478	14.046323
17.454954	1063.102646	14.051341
17.362075	1074.956012	14.056359
17.571335	1064.901287	14.061376
17.451461	1056.413491	14.066394
17.671872	1060.881990	14.071411
17.715695	1066.884924	14.076429
17.292910	1059.785044	14.081447
17.620282	1063.114309	14.086464
17.732440	1061.430301	14.091482
17.403431	1056.102316	14.096499
17.756318	1076.274474	14.101517
17.594517	1096.702745	14.106535
17.779360	1089.832700	14.111552
17.773697	1101.596490	14.116570
18.075051	1093.790612	14.121587
18.077782	1100.650895	14.126605
18.110255	1118.426865	14.131623
18.054282	1094.617785	14.136640
17.731703	1082.576976	14.141658
17.867665	1098.732946	14.146675
18.132202	1095.035803	14.151693
18.279288	1096.252908	14.156711
17.930278	1076.890550	14.161728
17.814839	1077.791255	14.166746
17.803290	1079.335703	14.171763
18.052221	1091.308551	14.176781
17.878609	1104.115082	14.181799
17.867788	1099.134138	14.186816
17.870044	1096.984807	14.191834
17.871306	1103.039958	14.196851
18.160039	1083.416325	14.201869
18.069199	1101.909386	14.206887
17.644970	1094.445420	14.211904
18.016091	1091.455149	14.216922
18.001491	1089.487117	14.221939
18.356221	1093.950060	14.226957
18.096555	1104.926242	14.231975
18.174253	1101.707339	14.236992
18.061407	1103.462983	14.242010
17.934332	1121.356055	14.247027
18.459786	1119.613290	14.252045
18.925503	1131.670995	14.257063
18.699012	1108.011115	14.262080
18.606963	1100.425139	14.267098
18.572425	1102.350489	14.272115
18.785809	1090.832813	14.277133
18.556599	1100.320157	14.282151
18.522552	1093.686838	14.287168
18.318395	1090.890827	14.292186
18.226854	1094.338331	14.297203
18.613795	1094.175083	14.302221
18.399120	1091.048386	14.307239
18.465683	1090.186830	14.312256
18.473884	1085.569418	14.317274
18.609309	1084.039311	14.322291
18.954831	1087.782440	14.327309
18.326182	1100.891486	14.332327
18.281646	1094.520289	14.337344
18.710010	1091.403452	14.342362
18.825288	1090.256334	14.347379
18.674703	1092.254001	14.352397
18.625183	1097.741458	14.357415
18.790394	1098.290721	14.362432
18.547204	1094.189964	14.367450
18.486757	1095.021947	14.372467
18.798973	1085.751141	14.377485
18.516544	1099.955336	14.382503
18.521273	1092.943232	14.387520
18.794230	1112.375821	14.392538
18.774223	1119.556548	14.397555
18.878590	1117.078385	14.402573
18.563601	1134.046583	14.407591
18.787847	1119.469334	14.412608
19.096336	1111.539651	14.417626
18.472700	1140.337193	14.422643
18.960006	1126.543298	14.427661
18.666909	1121.822933	14.432679
18.645413	1125.997132	14.437696
18.930635	1125.251186	14.442714
18.492883	1130.937237	14.447731
18.369146	1122.879401	14.452749
18.768070	1148.418539	14.457767
18.979521	1147.487178	14.462784
19.333993	1150.748215	14.467802
19.243003	1161.015378	14.472819
19.493279	1147.509804	14.477837
19.326732	1152.320870	14.482855
19.118671	1150.814846	14.487872
19.099751	1139.921053	14.492890
19.267092	1147.291073	14.497907
19.143046	1135.394354	14.502925
19.287987	1148.952477	14.507943
19.659962	1144.354644	14.512960
19.527009	1135.905476	14.517978
18.878161	1132.086866	14.522995
19.224884	1123.005972	14.528013
19.048558	1128.759039	14.533031
19.387426	1131.580008	14.538048
19.478116	1141.532538	14.543066
19.708759	1147.566334	14.548083
19.489428	1125.177277	14.553101
19.562584	1119.431198	14.558119
19.293882	1122.883776	14.563136
19.404312	1114.728793	14.568154
19.393061	1119.967062	14.573171
19.366446	1114.194369	14.578189
19.130540	1124.095560	14.583207
19.423065	1133.178257	14.588224
19.269077	1147.509474	14.593242
19.462142	1151.948567	14.598259
19.754852	1144.803629	14.603277
19.767517	1154.314411	14.608295
19.650545	1157.217994	14.613312
19.679177	1145.727658	14.618330
19.478042	1145.527753	14.623347
19.779841	1145.026074	14.628365
19.983726	1142.641482	14.633383
19.644960	1145.870446	14.638400
19.810196	1148.775810	14.643418
19.094621	1145.580720	14.648435
19.556786	1144.202288	14.653453
19.534224	1143.930952	14.658471
19.583921	1145.977601	14.663488
19.854349	1149.308619	14.668506
19.706558	1151.856921	14.673523
19.947177	1147.082993	14.678541
20.107931	1142.264793	14.683559
20.163797	1147.406561	14.688576
19.968953	1147.244390	14.693594
19.548348	1164.903191	14.698611
20.100008	1154.244574	14.703629
19.855558	1158.270024	14.708647
19.737736	1148.584301	14.713664
19.817775	1152.027083	14.718682
19.503038	1161.114690	14.723699
19.712561	1171.558738	14.728717
20.027739	1178.854941	14.733735
20.063872	1179.444431	14.738752
20.180915	1177.857914	14.743770
20.003369	1190.880288	14.748787
20.210948	1178.911808	14.753805
20.435566	1178.446106	14.758823
20.323428	1178.330494	14.763840
20.472529	1176.814454	14.768858
20.519099	1179.932709	14.773875
20.310101	1180.958901	14.778893
20.526543	1182.676083	14.783911
19.805626	1173.534027	14.788928
20.173226	1172.058443	14.793946
20.109485	1187.768453	14.798963
20.213764	1183.829902	14.803981
20.119655	1178.725514	14.808999
20.300817	1187.644393	14.814016
20.748723	1180.922537	14.819034
20.242199	1175.649726	14.824051
20.489655	1179.018792	14.829069
20.549250	1178.987578	14.834087
20.447449	1177.403765	14.839104
20.387855	1177.261362	14.844122
20.255218	1181.409264	14.849139
20.104171	1174.217780	14.854157
20.397844	1174.068960	14.859175
20.399472	1182.599462	14.864192
20.762566	1158.607271	14.869210
20.615457	1183.726744	14.874227
20.517989	1175.258504	14.879245
20.769791	1174.275403	14.884263
20.630673	1173.890081	14.889280
20.808290	1178.131570	14.894298
20.438875	1170.381193	14.899315
20.724394	1180.991399	14.904333
20.744124	1194.473222	14.909351
20.585987	1208.071246	14.914368
20.940894	1199.514067	14.919386
20.769015	1218.462516	14.924403
20.888351	1223.130707	14.929421
21.137366	1204.202350	14.934439
21.108705	1196.584398	14.939456
21.132450	1178.145193	14.944474
20.770565	1188.329798	14.949491
21.015463	1178.511295	14.954509
20.891745	1172.334813	14.959527
20.798391	1182.354390	14.964544
21.203447	1182.184605	14.969562
20.812412	1194.590007	14.974579
21.052171	1187.772250	14.979597
21.106785	1195.608486	14.984615
20.626953	1212.570748	14.989632
20.920433	1204.102641	14.994650
20.802920	1194.266469	14.999667
21.190469	1201.803833	15.004685
21.365082	1205.335312	15.009703
21.106125	1202.151747	15.014720
21.076182	1207.800746	15.019738
21.092424	1203.120562	15.024755
21.055520	1195.711813	15.029773
21.370405	1205.849150	15.034791
20.961720	1211.025981	15.039808
21.024128	1208.328002	15.044826
21.047989	1200.876734	15.049843
21.262742	1201.166083	15.054861
21.548448	1212.451761	15.059879
21.164533	1216.461500	15.064896
21.338635	1215.503045	15.069914
21.586740	1223.953280	15.074931
21.468245	1225.014708	15.079949
21.426349	1227.880903	15.084967
21.655402	1240.315150	15.089984
21.667909	1226.303413	15.095002
21.346969	1216.553394	15.100019
21.301502	1230.571724	15.105037
21.743982	1231.597136	15.110055
21.669033	1241.799114	15.115072
21.789833	1240.901623	15.120090
21.939352	1226.632834	15.125107
21.513304	1220.633831	15.130125
21.632612	1213.543102	15.135143
21.891961	1225.212217	15.140160
21.534689	1203.843120	15.145178
21.514026	1214.410064	15.150195
21.329736	1226.643947	15.155213
21.854559	1230.021316	15.160231
21.482440	1239.123174	15.165248
21.799223	1226.927983	15.170266
21.931210	1228.538279	15.175283
21.951937	1227.908466	15.180301
22.134304	1229.740124	15.185319
22.154104	1229.877664	15.190336
22.296571	1221.350657	15.195354
22.147381	1227.132736	15.200371
21.964567	1227.400199	15.205389
22.002130	1226.461748	15.210407
21.861368	1230.000277	15.215424
21.446096	1221.071815	15.220442
22.006854	1229.651460	15.225459
21.689884	1229.036907	15.230477
21.838403	1227.926798	15.235495
21.921820	1228.805476	15.240512
21.939003	1220.307243	15.245530
22.372998	1225.099197	15.250547
22.006486	1228.574456	15.255565
22.173284	1226.724241	15.260583
22.306399	1238.586049	15.265600
22.241344	1221.517942	15.270618
22.343257	1232.649391	15.275635
22.070378	1237.160191	15.280653
22.274872	1229.709961	15.285671
22.213108	1235.085729	15.290688
22.232657	1237.677050	15.295706
22.268952	1241.211319	15.300723
22.345423	1258.993369	15.305741
22.521496	1258.719910	15.310759
22.396283	1257.519819	15.315776
22.115514	1252.453337	15.320794
22.598598	1272.025000	15.325811
22.453428	1275.383390	15.330829
22.574535	1260.782704	15.335847
22.265277	1272.566089	15.340864
22.645609	1263.610444	15.345882
22.849096	1265.501008	15.350899
22.571067	1270.956221	15.355917
22.628808	1258.902417	15.360935
22.457727	1261.966315	15.365952
22.435823	1265.003988	15.370970
23.001694	1270.147924	15.375987
22.469541	1267.332274	15.381005
22.477663	1255.817887	15.386023
22.637620	1263.056330	15.391040
22.475190	1255.882631	15.396058
22.840254	1269.263169	15.401075
22.626711	1270.155888	15.406093
22.762099	1259.116452	15.411111
22.638625	1277.609212	15.416128
22.894099	1293.716115	15.421146
23.178741	1290.031940	15.426163
22.934127	1297.968652	15.431181
23.193705	1296.374117	15.436199
23.021494	1294.132151	15.441216
22.872572	1284.035602	15.446234
22.921489	1283.438131	15.451251
22.862567	1302.212530	15.456269
22.970792	1297.719644	15.461287
22.993155	1299.397268	15.466304
22.907443	1296.401163	15.471322
23.209505	1303.962348	15.476339
23.046253	1300.426582	15.481357
23.470674	1292.135971	15.486375
23.383384	1295.358640	15.491392
23.038903	1302.132907	15.496410
23.212377	1300.694508	15.501427
22.890510	1305.583248	15.506445
23.365222	1292.865527	15.511463
23.214397	1286.929663	15.516480
23.027949	1297.645103	15.521498
23.284198	1291.047770	15.526515
23.042297	1295.031896	15.531533
23.402788	1293.651753	15.536551
23.390431	1298.013828	15.541568
23.127604	1297.181499	15.546586
23.397141	1307.770816	15.551603
23.549581	1323.369858	15.556621
23.845675	1323.866994	15.561639
23.611805	1330.037062	15.566656
23.562838	1321.446374	15.571674
23.949127	1304.744466	15.576691
23.616124	1302.579849	15.581709
23.562488	1289.101345	15.586727
23.295676	1297.655211	15.591744
23.505802	1311.338511	15.596762
23.618151	1310.328650	15.601779
23.668126	1320.090613	15.606797
23.913553	1323.191191	15.611815
23.955020	1326.546307	15.616832
23.378195	1324.424142	15.621850
24.165794	1317.711241	15.626867
23.585644	1311.216095	15.631885
23.787367	1314.984815	15.636903
23.562773	1319.061545	15.641920
23.396566	1330.529649	15.646938
23.855417	1317.762175	15.651955
23.816792	1319.978143	15.656973
23.791994	1317.351240	15.661991
23.946975	1327.825663	15.667008
23.971419	1317.896870	15.672026
24.150208	1324.993079	15.677043
23.949228	1336.992246	15.682061
23.796988	1341.650831	15.687079
24.023061	1355.736001	15.692096
23.975705	1356.346183	15.697114
24.449051	1347.618192	15.702131
24.197555	1351.783616	15.707149
24.756816	1356.265192	15.712167
24.487171	1347.258860	15.717184
24.050689	1340.790740	15.722202
24.275520	1339.850859	15.727219
24.360741	1353.627267	15.732237
24.139866	1346.645636	15.737255
24.590936	1355.241116	15.742272
24.078894	1348.422346	15.747290
24.695224	1346.343329	15.752307
24.247273	1358.687411	15.757325
24.578207	1350.099864	15.762343
24.548334	1339.532494	15.767360
24.233243	1358.712032	15.772378
24.420752	1355.628646	15.777395
24.430033	1350.809825	15.782413
24.391326	1354.904462	15.787431
24.638669	1349.521776	15.792448
24.164632	1351.469595	15.797466
24.593509	1347.597227	15.802483
24.626612	1351.661298	15.807501
24.325731	1349.950154	15.812519
24.723848	1351.533609	15.817536
24.600384	1353.582724	15.822554
24.440245	1358.724633	15.827571
24.419356	1364.371012	15.832589
24.367271	1376.932130	15.837607
24.554163	1376.697230	15.842624
24.579274	1379.154802	15.847642
24.582583	1370.306076	15.852659
24.705029	1385.738511	15.857677
24.678810	1372.186123	15.862695
24.888151	1378.130631	15.867712
24.620582	1397.876688	15.872730
24.928877	1402.218674	15.877747
24.933686	1409.599342	15.882765
24.808082	1412.975983	15.887783
25.148203	1418.860515	15.892800
24.986723	1413.433767	15.897818
25.351672	1403.711013	15.902835
25.057177	1417.201065	15.907853
24.507803	1410.165831	15.912871
25.121425	1403.577495	15.917888
24.846991	1409.161670	15.922906
25.106729	1400.950372	15.927923
25.155846	1402.921376	15.932941
25.318447	1420.991500	15.937959
25.625729	1411.400496	15.942976
25.265457	1412.428279	15.947994
25.412165	1397.478599	15.953011
25.900204	1401.741481	15.958029
25.433076	1405.815209	15.963047
25.792940	1395.504608	15.968064
25.645516	1407.219628	15.973082
25.622297	1406.187879	15.978099
25.522714	1405.863330	15.983117
25.634694	1412.591149	15.988135
25.557177	1402.917106	15.993152
25.506901	1405.241099	15.998170
25.849708	1405.462645	16.003187
25.566349	1401.601676	16.008205
25.520915	1394.834106	16.013223
25.370125	1400.165597	16.018240
25.602403	1410.115175	16.023258
25.486444	1393.772308	16.028275
25.646180	1410.761166	16.033293
25.611915	1432.845722	16.038311
25.682986	1430.261610	16.043328
25.720578	1431.673778	16.048346
25.557768	1434.960129	16.053363
25.860884	1442.208263	16.058381
25.732361	1439.957087	16.063399
26.065872	1432.892663	16.068416
25.506837	1443.519599	16.073434
25.865764	1443.560358	16.078451
25.994485	1433.854578	16.083469
25.972032	1436.766213	16.088487
25.899458	1436.828678	16.093504
25.671429	1443.554437	16.098522
25.876933	1452.124615	16.103539
25.925416	1460.320411	16.108557
26.078019	1461.959604	16.113575
26.553416	1468.472888	16.118592
26.106508	1471.415109	16.123610
26.332961	1463.397046	16.128627
26.439821	1475.490311	16.133645
25.977263	1475.986655	16.138663
26.389092	1464.776409	16.143680
26.170443	1471.961980	16.148698
26.146096	1470.087426	16.153715
26.393866	1458.480932	16.158733
26.025993	1467.833170	16.163751
26.319177	1466.684771	16.168768
26.211912	1463.007649	16.173786
26.444105	1468.303431	16.178803
26.510642	1474.663447	16.183821
26.299033	1464.803090	16.188839
26.615601	1479.901616	16.193856
26.630091	1489.043066	16.198874
26.590874	1498.533504	16.203891
26.493640	1489.545639	16.208909
26.744480	1492.108623	16.213927
26.602404	1489.337708	16.218944
26.090695	1502.420879	16.223962
26.372008	1492.942762	16.228979
26.522938	1492.173526	16.233997
26.890602	1500.034160	16.239015
27.263565	1492.369573	16.244032
27.161462	1490.918436	16.249050
27.160584	1502.927178	16.254067
26.998104	1494.707266	16.259085
26.928855	1496.269951	16.264103
27.189003	1495.735386	16.269120
27.237235	1498.410778	16.274138
26.993879	1501.083379	16.279155
27.153221	1498.733451	16.284173
27.162595	1494.891792	16.289191
27.241182	1484.749249	16.294208
26.941716	1498.908995	16.299226
26.767568	1499.753884	16.304243
27.122907	1490.402689	16.309261
26.986323	1494.942019	16.314279
27.455755	1489.602691	16.319296
27.125983	1490.188297	16.324314
27.170881	1487.707502	16.329331
26.985501	1488.664269	16.334349
27.000527	1489.497382	16.339367
27.308631	1483.928453	16.344384
27.273496	1492.657891	16.349402
27.055086	1514.312823	16.354419
26.993043	1520.428986	16.359437
26.698348	1529.114734	16.364455
27.090303	1525.050420	16.369472
27.276403	1528.732417	16.374490
27.320192	1536.224600	16.379507
27.540692	1542.333644	16.384525
27.661175	1564.729777	16.389543
27.850248	1561.354794	16.394560
27.837775	1559.512514	16.399578
27.593779	1556.772796	16.404595
27.686114	1541.590263	16.409613
27.426368	1557.451133	16.414631
27.748236	1566.438306	16.419648
27.808415	1562.813990	16.424666
27.658620	1559.935495	16.429683
27.794509	1557.873450	16.434701
27.621184	1563.850167	16.439719
28.013972	1556.934136	16.444736
27.626652	1559.699818	16.449754
27.728098	1558.944464	16.454771
27.977467	1558.474268	16.459789
27.424656	1569.232133	16.464807
27.375143	1571.673725	16.469824
27.831174	1580.421837	16.474842
28.007170	1587.928611	16.479859
28.390350	1596.369326	16.484877
28.018505	1603.279724	16.489895
28.300776	1587.090894	16.494912
28.229117	1603.948541	16.499930
28.354684	1601.416607	16.504947
28.474209	1592.090738	16.509965
28.298141	1592.493096	16.514983
28.216317	1595.085680	16.520000
28.465116	1588.143240	16.525018
28.246498	1591.770493	16.530035
28.272474	1591.482862	16.535053
28.299696	1589.147274	16.540071
28.285966	1588.253296	16.545088
28.257584	1595.841675	16.550106
28.434881	1595.477274	16.555123
28.378401	1587.101822	16.560141
28.154076	1592.995456	16.565159
28.251855	1595.404642	16.570176
28.465775	1591.068394	16.575194
28.285695	1597.549124	16.580211
28.881995	1611.645977	16.585229
28.801523	1618.887906	16.590247
28.973281	1618.941488	16.595264
28.910625	1624.072100	16.600282
28.468327	1621.134856	16.605299
28.601143	1624.367081	16.610317
28.664779	1630.340489	16.615335
28.820162	1628.568284	16.620352
29.006563	1619.833431	16.625370
28.685062	1618.728928	16.630387
28.890025	1622.541079	16.635405
28.766921	1630.099662	16.640423
28.909719	1613.902753	16.645440
28.848929	1626.891439	16.650458
28.790961	1625.076942	16.655475
29.195394	1619.181655	16.660493
28.751226	1628.327730	16.665511
28.662131	1626.944106	16.670528
29.092936	1637.393631	16.675546
29.274714	1643.638426	16.680563
29.307335	1650.030887	16.685581
29.434897	1646.231659	16.690599
29.399332	1641.575846	16.695616
29.302746	1645.002656	16.700634
29.246561	1658.190975	16.705651
29.478592	1644.439393	16.710669
29.519199	1648.620397	16.715687
29.504434	1652.960926	16.720704
29.456081	1652.209065	16.725722
29.412967	1648.464218	16.730739
29.775436	1653.678702	16.735757
29.525170	1639.859796	16.740775
29.371353	1649.931001	16.745792
29.408322	1656.592395	16.750810
29.648877	1648.109764	16.755827
29.551499	1631.362446	16.760845
29.414819	1650.398313	16.765863
29.459067	1648.902507	16.770880
29.721023	1644.199103	16.775898
29.575035	1658.836124	16.780915
29.866374	1650.605498	16.785933
29.767512	1653.012743	16.790951
29.604160	1646.109647	16.795968
29.794473	1659.840227	16.800986
29.616452	1678.191909	16.806003
29.955925	1676.141476	16.811021
29.793232	1687.380357	16.816039
29.946377	1688.681143	16.821056
30.335952	1682.813679	16.826074
30.003893	1678.241491	16.831091
30.105756	1676.538156	16.836109
29.752507	1679.510995	16.841127
29.871886	1675.989257	16.846144
30.295054	1679.352821	16.851162
29.924709	1676.807167	16.856179
30.072845	1671.662781	16.861197
29.986844	1680.900271	16.866215
29.931462	1697.657508	16.871232
30.170761	1702.721322	16.876250
30.270078	1714.125363	16.881267
30.536727	1710.447999	16.886285
30.832699	1703.014113	16.891303
30.455906	1720.444683	16.896320
30.865601	1707.060290	16.901338
30.411414	1697.087920	16.906355
30.902367	1692.172865	16.911373
30.470411	1692.698405	16.916391
30.253631	1676.309899	16.921408
30.764819	1686.352919	16.926426
30.516694	1704.855766	16.931443
30.944150	1699.173152	16.936461
30.815367	1706.560686	16.941479
30.748468	1707.592364	16.946496
30.901619	1698.198678	16.951514
30.467703	1686.861135	16.956531
30.380089	1700.138727	16.961549
30.724010	1707.300135	16.966567
30.468924	1698.230176	16.971584
30.575336	1701.756113	16.976602
30.475019	1703.018086	16.981619
30.495271	1699.122617	16.986637
30.877680	1725.646615	16.991655
30.870521	1726.278905	16.996672
31.363473	1726.152459	17.001690
30.939051	1730.094820	17.006707
30.965641	1728.238978	17.011725
30.951091	1732.892446	17.016743
30.871875	1725.949037	17.021760
31.086447	1724.138697	17.026778
30.971811	1727.637594	17.031795
31.426152	1727.955464	17.036813
31.578127	1722.578567	17.041831
31.220920	1737.763296	17.046848
31.527905	1721.620038	17.051866
31.293132	1740.786581	17.056883
31.110018	1732.242040	17.061901
31.567857	1747.037796	17.066919
31.538727	1756.716269	17.071936
31.534527	1765.625371	17.076954
31.894940	1761.998241	17.081971
31.996158	1753.297859	17.086989
31.768330	1744.075749	17.092007
31.366717	1731.161382	17.097024
31.699106	1742.083286	17.102042
31.766085	1762.610441	17.107059
31.862628	1759.398325	17.112077
31.693219	1761.350965	17.117095
31.831182	1773.536556	17.122112
32.206012	1760.826298	17.127130
31.938838	1760.498141	17.132147
32.021588	1758.565701	17.137165
31.784938	1743.092103	17.142183
31.464428	1762.647005	17.147200
31.908159	1759.743219	17.152218
31.688619	1764.440214	17.157235
32.098936	1775.957652	17.162253
32.104467	1759.915343	17.167271
31.931167	1762.657306	17.172288
32.187119	1770.087185	17.177306
32.151446	1762.245141	17.182323
32.143828	1763.413465	17.187341
31.957154	1771.585694	17.192359
32.150919	1778.655035	17.197376
32.416068	1763.697238	17.202394
32.081982	1770.324340	17.207411
32.169925	1787.001305	17.212429
32.379426	1791.283163	17.217447
32.263510	1799.590744	17.222464
32.446577	1791.605859	17.227482
32.691732	1795.777311	17.232499
32.768104	1792.824001	17.237517
32.614121	1786.075181	17.242535
32.449312	1798.282481	17.247552
32.796130	1799.945121	17.252570
32.544011	1792.594678	17.257587
32.216255	1796.012090	17.262605
32.524201	1787.665865	17.267623
32.591707	1797.028235	17.272640
32.674186	1784.183614	17.277658
32.432885	1799.360863	17.282675
32.688339	1792.392628	17.287693
32.910676	1790.624693	17.292711
32.419219	1807.287005	17.297728
32.937031	1818.627479	17.302746
33.177371	1823.715370	17.307763
33.096150	1819.967135	17.312781
33.105663	1827.558420	17.317799
32.903688	1828.129809	17.322816
33.102929	1818.130475	17.327834
33.107024	1818.778230	17.332851
33.157530	1819.285262	17.337869
33.437548	1816.413242	17.342887
33.240955	1824.301150	17.347904
33.232505	1811.576637	17.352922
33.642922	1828.052935	17.357939
33.126182	1829.108372	17.362957
33.638341	1818.073592	17.367975
33.495501	1813.261853	17.372992
33.216616	1820.625432	17.378010
33.462872	1820.738153	17.383027
33.649694	1819.986589	17.388045
33.535086	1811.955620	17.393063
33.479006	1818.762759	17.398080
33.554027	1816.739278	17.403098
33.648552	1808.770787	17.408115
33.390747	1812.744683	17.413133
33.454625	1818.035727	17.418151
33.498914	1814.564747	17.423168
33.335744	1818.865484	17.428186
33.568867	1822.765737	17.433203
33.731173	1841.933710	17.438221
33.586762	1843.171686	17.443239
33.596301	1844.981000	17.448256
33.730697	1829.874885	17.453274
34.185524	1840.632746	17.458291
33.775025	1839.897023	17.463309
33.914359	1835.494106	17.468327
34.115050	1837.176568	17.473344
34.104120	1831.081565	17.478362
34.105038	1829.205351	17.483379
33.997454	1842.910526	17.488397
34.314866	1821.343658	17.493415
33.919688	1829.453731	17.498432
34.440938	1850.106503	17.503450
34.547700	1853.266123	17.508467
34.542024	1851.651003	17.513485
34.455451	1837.350003	17.518503
34.410235	1828.014605	17.523520
34.408227	1829.615615	17.528538
34.644073	1830.509095	17.533555
34.463767	1841.312075	17.538573
34.624159	1820.952507	17.543591
34.740834	1839.238166	17.548608
34.593455	1841.940825	17.553626
34.559848	1827.456890	17.558643
34.381602	1852.045850	17.563661
34.786554	1850.489042	17.568679
34.633836	1856.655160	17.573696
34.715010	1860.302809	17.578714
34.840706	1855.669097	17.583731
34.773183	1852.697039	17.588749
35.028329	1850.030870	17.593767
34.787092	1866.222225	17.598784
34.711865	1852.912130	17.603802
35.104194	1852.139006	17.608819
34.924268	1874.328372	17.613837
34.829267	1860.354492	17.618855
35.267656	1849.128165	17.623872
34.969366	1856.062145	17.628890
35.090463	1864.138099	17.633907
35.177291	1860.656339	17.638925
35.289053	1849.381045	17.643943
35.085147	1856.223848	17.648960
35.382397	1861.698954	17.653978
35.388136	1859.695773	17.658995
35.014735	1863.996227	17.664013
35.268141	1851.205579	17.669031
35.133244	1850.307792	17.674048
34.886400	1873.560056	17.679066
35.554936	1880.643892	17.684083
35.372371	1881.948208	17.689101
35.644166	1894.091702	17.694119
35.201847	1894.988406	17.699136
35.248183	1887.461251	17.704154
35.809240	1877.315092	17.709171
35.256351	1891.819598	17.714189
35.330887	1889.096467	17.719207
35.463649	1908.210947	17.724224
35.663749	1931.207180	17.729242
35.951125	1921.818734	17.734259
36.002751	1916.802603	17.739277
35.744289	1917.779937	17.744295
35.828003	1913.592266	17.749312
35.944571	1921.513898	17.754330
35.858603	1905.975870	17.759347
35.584116	1913.687938	17.764365
35.946699	1908.699550	17.769383
35.785967	1921.583360	17.774400
36.158681	1928.362796	17.779418
36.386795	1935.074802	17.784435
35.902731	1939.244762	17.789453
36.249547	1948.895086	17.794471
35.936448	1942.854498	17.799488
36.229352	1940.403309	17.804506
36.268044	1935.046043	17.809523
36.248135	1946.862235	17.814541
36.245741	1934.692265	17.819559
36.043272	1937.600871	17.824576
36.381625	1948.590629	17.829594
36.857359	1948.577842	17.834611
36.917227	1947.344553	17.839629
36.643191	1943.843479	17.844647
36.794677	1936.343211	17.849664
36.328997	1937.858469	17.854682
36.264999	1948.367730	17.859699
36.621349	1963.034024	17.864717
36.877202	1965.839344	17.869735
37.172533	1963.700707	17.874752
37.165439	1965.350597	17.879770
37.287054	1947.762902	17.884787
37.232909	1966.789850	17.889805
37.609865	1942.901227	17.894823
37.239745	1926.910388	17.899840
37.039618	1928.181983	17.904858
37.352078	1917.795415	17.909875
37.227814	1921.998227	17.914893
37.073620	1920.349381	17.919911
37.649942	1927.597475	17.924928
37.168120	1922.144948	17.929946
37.645423	1916.407568	17.934963
37.664085	1926.885637	17.939981
37.698365	1922.312674	17.944999
37.390826	1921.560918	17.950016
37.516404	1924.127354	17.955034
37.610851	1915.481340	17.960051
37.509639	1922.241856	17.965069
37.604186	1916.475806	17.970087
37.812823	1918.567152	17.975104
37.500977	1918.757140	17.980122
37.834118	1920.103391	17.985139
37.399680	1927.234093	17.990157
37.460957	1925.142602	17.995175
37.894517	1921.243535	18.000192
37.600653	1925.291717	18.005210
37.818375	1916.328910	18.010227
37.579542	1926.480084	18.015245
37.539974	1918.795672	18.020263
37.678694	1916.282574	18.025280
37.227482	1935.590230	18.030298
37.979821	1942.523254	18.035315
38.021205	1942.339357	18.040333
37.961964	1963.982591	18.045351
37.842161	1949.303558	18.050368
38.010137	1949.678793	18.055386
37.954550	1953.184516	18.060403
37.504283	1960.053313	18.065421
37.689544	1977.145062	18.070439
38.021988	1972.849352	18.075456
38.267248	1987.720621	18.080474
38.608698	1979.510277	18.085491
38.332850	1997.730883	18.090509
38.388266	1994.950467	18.095527
38.411254	1993.928167	18.100544
38.081663	1983.519713	18.105562
38.639962	1988.253380	18.110579
38.400794	1990.457116	18.115597
38.409102	1991.739545	18.120615
38.746451	2009.841712	18.125632
38.887814	2025.816681	18.130650
39.074244	2018.171441	18.135667
38.952554	2018.313276	18.140685
38.759034	2016.271947	18.145703
38.863424	2007.237076	18.150720
38.968721	2021.233771	18.155738
38.985018	2016.791100	18.160755
39.030973	2019.891519	18.165773
39.104393	2023.806995	18.170791
39.210155	2017.797742	18.175808
38.949085	2016.976891	18.180826
39.062824	2017.065848	18.185843
39.340175	2020.801577	18.190861
39.109284	2030.240364	18.195879
39.161189	2020.337483	18.200896
39.172008	2022.441850	18.205914
39.353336	2030.182776	18.210931
39.245990	2017.045349	18.215949
39.303122	2014.853951	18.220967
39.391577	2016.565608	18.225984
38.878479	2020.370743	18.231002
39.011270	2023.174560	18.236019
39.286724	2037.120713	18.241037
39.481690	2033.929476	18.246055
39.938705	2031.346638	18.251072
39.546067	2048.668593	18.256090
39.738753	2035.851609	18.261107
40.019783	2041.830587	18.266125
40.019512	2042.873125	18.271143
39.685006	2040.863160	18.276160
39.480123	2042.957312	18.281178
40.050920	2034.823594	18.286195
39.936465	2039.473390	18.291213
39.823928	2039.144866	18.296231
40.075634	2030.536181	18.301248
39.891192	2034.675156	18.306266
39.905034	2037.303574	18.311283
40.241297	2035.841161	18.316301
40.070946	2042.716292	18.321319
40.471836	2034.732488	18.326336
40.404275	2032.454421	18.331354
40.288267	2043.764774	18.336371
40.504427	2028.400098	18.341389
39.955726	2041.800825	18.346407
40.156146	2054.273136	18.351424
40.362896	2060.343520	18.356442
40.587753	2057.324092	18.361459
40.797888	2074.218946	18.366477
40.582572	2076.646288	18.371495
40.565424	2061.309110	18.376512
40.747244	2072.294905	18.381530
40.620883	2060.849379	18.386547
40.834234	2059.471834	18.391565
40.419288	2062.419708	18.396583
40.871188	2062.167579	18.401600
40.379317	2070.330366	18.406618
40.845540	2059.064055	18.411635
41.075071	2066.030581	18.416653
40.818098	2068.408709	18.421671
40.869159	2063.454626	18.426688
40.633482	2074.239952	18.431706
40.848156	2080.589715	18.436723
41.201363	2094.291402	18.441741
41.263315	2087.987621	18.446759
41.349595	2091.082178	18.451776
41.580226	2096.863031	18.456794
41.276035	2095.334415	18.461811
41.345508	2090.396177	18.466829
41.270266	2099.594938	18.471847
41.424526	2087.260589	18.476864
41.163050	2095.184551	18.481882
41.191593	2091.648008	18.486899
41.652882	2083.714034	18.491917
41.271369	2093.744225	18.496935
41.338144	2110.121526	18.501952
41.449917	2114.786711	18.506970
41.593089	2122.760738	18.511987
42.022401	2122.603277	18.517005
41.709171	2113.713134	18.522023
41.977618	2114.516017	18.527040
41.816900	2131.358448	18.532058
42.005662	2126.883507	18.537075
42.038845	2119.348570	18.542093
41.901014	2118.900419	18.547111
42.088256	2120.875853	18.552128
42.039072	2122.175862	18.557146
42.172787	2123.743256	18.562163
42.300763	2130.018791	18.567181
42.316060	2121.829003	18.572199
42.497176	2122.240454	18.577216
42.208511	2124.779716	18.582234
42.150071	2120.803650	18.587251
42.209988	2115.510129	18.592269
41.866261	2126.348580	18.597287
42.352793	2117.814416	18.602304
42.582170	2152.293934	18.607322
42.609469	2144.103725	18.612339
42.760809	2145.127909	18.617357
42.912762	2148.731848	18.622375
43.092637	2137.786196	18.627392
42.829285	2121.909780	18.632410
43.051300	2116.660528	18.637427
42.572915	2110.762136	18.642445
42.632831	2112.808407	18.647463
43.079934	2112.973957	18.652480
42.793213	2114.322469	18.657498
42.479443	2120.444446	18.662515
42.780287	2124.322957	18.667533
42.954572	2137.955835	18.672551
42.785840	2142.694347	18.677568
42.505956	2137.670530	18.682586
42.632234	2148.752163	18.687603
43.106263	2159.005945	18.692621
43.198502	2170.459913	18.697639
43.106381	2171.416073	18.702656
43.405760	2170.815956	18.707674
43.308232	2161.300437	18.712691
43.625972	2164.146152	18.717709
43.691449	2177.547070	18.722727
43.833684	2170.993595	18.727744
43.910988	2169.505464	18.732762
43.607854	2171.791836	18.737779
43.844874	2164.707201	18.742797
43.774009	2173.333490	18.747815
43.737704	2175.058105	18.752832
43.967365	2159.342874	18.757850
43.480750	2162.559670	18.762867
43.972780	2167.554713	18.767885
43.654864	2176.924513	18.772903
43.796958	2155.909523	18.777920
43.749539	2163.626117	18.782938
43.193604	2165.798963	18.787955
43.919991	2179.553222	18.792973
43.980519	2189.606483	18.797991
43.939793	2198.028218	18.803008
44.044083	2203.187335	18.808026
44.144532	2191.834732	18.813043
44.301414	2194.512368	18.818061
44.425952	2197.705732	18.823079
44.369423	2197.531319	18.828096
44.410726	2194.601639	18.833114
44.395817	2202.189862	18.838131
44.526681	2195.159562	18.843149
44.397909	2184.651849	18.848167
44.442636	2207.479701	18.853184
44.722949	2214.077111	18.858202
44.892066	2229.004301	18.863219
45.004081	2213.846003	18.868237
45.042957	2228.313068	18.873255
45.200687	2198.601590	18.878272
45.220044	2189.045481	18.883290
45.237468	2179.867219	18.888307
45.046788	2172.235011	18.893325
45.211193	2180.903324	18.898343
45.342024	2177.433315	18.903360
45.325826	2183.305771	18.908378
45.008500	2170.403481	18.913395
45.096673	2174.779504	18.918413
44.695460	2177.641280	18.923431
44.859983	2174.166097	18.928448
45.134444	2194.894756	18.933466
45.272376	2214.961031	18.938483
45.547525	2209.766545	18.943501
45.810881	2213.666036	18.948519
45.293091	2216.255772	18.953536
45.635315	2205.298204	18.958554
45.304172	2201.527203	18.963571
45.566034	2211.517487	18.968589
45.590655	2208.980878	18.973607
45.429569	2212.498188	18.978624
45.602519	2213.163722	18.983642
45.054355	2216.793810	18.988659
45.634593	2205.709123	18.993677
45.400473	2219.231034	18.998695
45.753883	2241.253670	19.003712
46.024725	2238.277784	19.008730
45.712817	2235.667856	19.013747
45.964861	2226.081737	19.018765
45.495077	2233.776831	19.023783
45.661610	2230.766220	19.028800
46.138877	2245.856856	19.033818
46.316470	2262.140030	19.038835
46.534787	2242.083298	19.043853
46.811999	2257.852809	19.048871
46.621680	2256.849403	19.053888
46.758556	2253.153990	19.058906
46.533477	2243.564231	19.063923
46.667616	2236.679027	19.068941
46.421332	2232.419435	19.073959
46.624776	2242.872696	19.078976
46.670951	2253.619052	19.083994
46.495325	2252.047721	19.089011
46.706010	2249.138265	19.094029
46.811415	2251.812213	19.099047
46.924303	2252.241635	19.104064
47.163054	2244.294358	19.109082
47.293557	2251.531638	19.114099
47.419593	2245.600042	19.119117
46.909808	2249.771578	19.124135
46.837734	2244.596468	19.129152
47.544537	2242.902940	19.134170
46.870981	2255.781031	19.139187
47.373661	2256.619225	19.144205
47.251137	2259.929405	19.149223
47.158764	2255.839040	19.154240
47.475308	2257.636447	19.159258
47.309009	2255.331950	19.164275
47.328266	2256.295692	19.169293
47.318458	2261.419161	19.174311
47.111687	2255.672267	19.179328
47.535990	2261.529239	19.184346
47.639203	2283.956238	19.189363
47.514781	2278.178997	19.194381
47.548295	2285.457516	19.199399
47.114269	2300.539752	19.204416
47.556990	2284.871266	19.209434
47.593050	2283.506858	19.214451
47.615705	2303.888333	19.219469
47.881681	2312.915689	19.224487
47.974710	2313.126957	19.229504
48.350377	2306.220117	19.234522
48.142365	2311.922564	19.239539
48.049826	2307.447209	19.244557
48.236284	2309.025195	19.249575
48.289605	2304.318867	19.254592
48.524788	2304.651317	19.259610
48.192253	2307.764735	19.264627
48.306117	2306.558319	19.269645
48.468159	2306.846561	19.274663
48.460583	2291.360342	19.279680
48.459741	2293.427306	19.284698
48.614702	2300.937315	19.289715
48.427727	2293.108783	19.294733
48.520283	2301.375886	19.299751
48.328860	2304.434886	19.304768
48.701695	2308.838310	19.309786
48.632514	2324.003575	19.314803
49.059419	2329.115132	19.319821
48.862893	2324.113500	19.324839
49.080562	2338.700914	19.329856
48.885806	2321.445756	19.334874
49.030247	2329.422239	19.339891
49.070655	2331.677846	19.344909
49.058163	2332.893274	19.349927
49.197578	2334.127100	19.354944
49.412384	2321.310555	19.359962
49.163958	2337.038671	19.364979
49.467562	2325.268378	19.369997
49.398938	2326.349196	19.375015
49.133924	2335.149180	19.380032
49.409780	2320.915586	19.385050
49.159401	2340.082498	19.390067
49.383506	2358.159108	19.395085
49.710489	2351.644117	19.400103
49.757825	2360.152561	19.405120
49.886490	2362.840991	19.410138
49.860500	2361.217759	19.415155
50.237058	2360.624762	19.420173
50.422552	2361.435067	19.425191
49.681148	2353.309769	19.430208
49.839541	2350.834292	19.435226
49.919887	2360.533436	19.440243
50.161360	2345.757911	19.445261
50.278739	2346.562937	19.450279
50.043957	2362.674814	19.455296
50.474532	2350.903991	19.460314
50.434130	2346.072993	19.465331
50.390974	2348.604396	19.470349
50.218845	2353.212443	19.475367
49.870631	2358.542440	19.480384
50.561355	2360.654374	19.485402
50.523545	2370.240186	19.490419
49.903108	2380.300398	19.495437
50.483436	2381.865665	19.500455
50.494448	2392.452391	19.505472
50.924918	2384.034227	19.510490
50.677786	2382.166654	19.515507
50.631852	2394.808875	19.520525
50.917742	2384.836390	19.525543
51.058408	2393.111732	19.530560
50.967361	2382.223863	19.535578
51.098250	2388.243533	19.540595
50.834994	2399.320626	19.545613
51.063018	2408.592282	19.550631
51.347334	2410.897550	19.555648
51.729049	2411.268776	19.560666
51.234543	2417.474273	19.565683
51.160684	2412.449390	19.570701
51.390885	2408.372801	19.575719
51.236204	2428.496958	19.580736
51.536640	2409.408641	19.585754
51.604185	2412.981909	19.590771
51.468815	2414.057032	19.595789
51.674765	2401.102920	19.600807
51.688309	2411.681762	19.605824
51.828901	2403.160910	19.610842
51.738440	2409.728539	19.615859
51.718046	2413.823185	19.620877
52.140683	2404.515631	19.625895
51.722242	2418.140806	19.630912
51.627987	2415.302573	19.635930
52.164614	2421.676434	19.640947
52.015335	2436.964682	19.645965
52.379150	2435.267974	19.650983
52.243832	2432.593794	19.656000
52.040514	2432.293647	19.661018
52.532990	2433.460676	19.666035
52.118626	2429.102830	19.671053
52.528728	2432.407900	19.676071
52.138695	2444.782247	19.681088
52.274547	2442.964756	19.686106
52.395818	2438.515641	19.691123
52.200043	2426.306574	19.696141
52.434190	2438.427983	19.701159
52.587779	2469.236393	19.706176
53.028691	2469.731292	19.711194
52.906689	2457.408444	19.716211
52.400056	2463.000856	19.721229
52.986078	2464.405952	19.726247
52.663459	2463.010254	19.731264
52.990145	2456.636399	19.736282
52.877043	2466.720499	19.741299
52.845366	2465.099574	19.746317
53.176261	2448.677810	19.751335
53.147339	2489.621107	19.756352
52.955355	2489.534816	19.761370
53.201969	2488.988483	19.766387
53.099088	2508.790429	19.771405
53.307050	2491.834450	19.776423
53.513707	2484.991282	19.781440
53.356526	2481.622731	19.786458
53.568192	2486.172908	19.791475
53.572281	2497.677510	19.796493
53.747847	2501.093590	19.801511
53.921096	2511.847865	19.806528
54.188309	2518.059412	19.811546
54.205395	2511.307790	19.816563
53.848934	2511.253403	19.821581
54.397781	2511.565126	19.826599
54.541443	2496.002928	19.831616
54.586017	2473.125028	19.836634
54.454335	2470.523660	19.841651
54.195288	2474.736099	19.846669
54.342208	2471.944807	19.851687
54.400131	2477.495899	19.856704
54.282552	2469.637702	19.861722
54.315275	2473.649380	19.866739
54.323494	2473.632361	19.871757
54.516436	2490.762188	19.876775
54.616394	2506.801776	19.881792
54.153593	2508.027854	19.886810
54.721312	2493.624032	19.891827
54.509316	2508.063923	19.896845
54.572411	2507.054055	19.901863
54.361997	2511.439753	19.906880
54.116659	2507.005138	19.911898
54.828608	2519.895229	19.916915
54.862897	2533.021316	19.921933
55.044816	2523.941249	19.926951
54.955950	2530.005555	19.931968
55.090400	2537.174212	19.936986
55.595558	2529.669345	19.942003
55.122351	2524.962560	19.947021
55.179210	2523.033714	19.952039
55.397544	2533.436684	19.957056
55.522411	2528.964115	19.962074
55.452037	2520.569392	19.967091
55.470741	2536.091966	19.972109
55.612412	2550.826381	19.977127
55.860970	2558.347032	19.982144
55.591034	2563.901154	19.987162
55.615271	2557.800250	19.992179
55.576527	2559.228089	19.997197
56.010933	2553.160188	20.002215
55.577167	2557.607608	20.007232
55.542270	2562.617220	20.012250
55.921929	2555.750749	20.017267
56.119814	2563.798043	20.022285
56.227275	2548.370504	20.027303
56.343942	2561.907775	20.032320
56.362795	2578.481273	20.037338
56.773463	2569.937944	20.042355
56.193165	2561.102696	20.047373
56.380892	2568.269847	20.052391
56.872410	2584.626675	20.057408
56.468656	2576.938143	20.062426
56.724538	2575.597223	20.067443
56.347899	2584.095541	20.072461
56.424117	2570.700750	20.077479
56.782755	2585.158025	20.082496
56.746065	2584.909468	20.087514
56.796029	2581.783023	20.092531
57.114454	2575.812423	20.097549
57.037424	2587.231684	20.102567
56.953373	2574.991638	20.107584
56.940544	2581.182562	20.112602
57.143409	2572.752697	20.117619
57.218253	2600.206126	20.122637
57.560422	2614.253778	20.127655
57.175545	2614.492253	20.132672
57.069566	2614.259870	20.137690
57.196059	2610.994797	20.142707
57.114025	2620.743573	20.147725
57.347099	2609.137071	20.152743
57.445775	2614.359061	20.157760
57.348089	2626.288224	20.162778
57.502835	2615.311547	20.167795
57.983376	2632.830590	20.172813
58.061950	2632.140575	20.177831
58.193270	2615.181772	20.182848
58.087254	2625.374443	20.187866
58.480798	2628.744296	20.192883
58.120399	2632.250545	20.197901
58.269578	2623.648828	20.202919
58.330174	2624.992939	20.207936
58.106102	2625.178860	20.212954
58.241363	2618.041745	20.217971
58.243332	2620.954488	20.222989
58.182868	2616.046804	20.228007
58.619625	2620.466527	20.233024
58.662149	2613.457918	20.238042
58.765755	2614.882120	20.243059
58.248405	2630.464040	20.248077
58.655384	2635.174297	20.253095
58.456409	2637.214997	20.258112
58.686921	2654.697040	20.263130
58.546363	2648.469798	20.268147
58.259529	2648.991068	20.273165
58.940361	2644.765944	20.278183
59.037252	2651.737726	20.283200
59.372108	2670.808734	20.288218
59.205714	2670.544209	20.293235
59.227783	2652.573764	20.298253
59.275267	2666.765230	20.303271
59.353719	2673.917813	20.308288
59.476108	2676.874838	20.313306
59.781879	2669.345965	20.318323
59.739838	2672.896656	20.323341
59.569216	2676.483949	20.328359
60.037349	2664.795456	20.333376
59.438177	2663.961544	20.338394
59.543670	2670.822472	20.343411
60.045334	2670.703641	20.348429
59.963476	2668.219785	20.353447
60.014894	2674.218055	20.358464
59.813992	2671.998145	20.363482
59.943425	2673.215539	20.368499
60.019477	2675.390312	20.373517
60.254796	2678.413513	20.378535
59.997530	2672.576979	20.383552
59.876686	2683.217777	20.388570
60.352309	2682.675324	20.393587
60.327920	2696.650954	20.398605
60.194168	2697.495923	20.403623
60.654225	2701.875207	20.408640
60.402935	2694.321648	20.413658
60.439546	2700.420400	20.418675
60.482909	2703.788100	20.423693
60.172244	2714.888408	20.428711
60.559226	2720.072241	20.433728
60.653865	2730.936306	20.438746
61.087205	2724.270720	20.443763
61.319521	2723.071468	20.448781
61.072450	2725.873621	20.453799
61.208860	2729.921773	20.458816
61.139136	2729.311767	20.463834
61.356705	2713.447786	20.468851
61.605407	2719.965801	20.473869
61.572399	2719.879221	20.478887
61.874877	2713.996237	20.483904
61.510155	2721.011260	20.488922
61.714431	2716.034603	20.493939
61.586187	2718.903729	20.498957
61.598597	2719.715097	20.503975
61.882298	2720.426917	20.508992
61.781188	2720.629132	20.514010
61.948712	2719.492159	20.519027
61.832661	2717.764290	20.524045
61.834810	2729.656171	20.529063
62.002798	2722.552180	20.534080
61.661737	2754.018056	20.539098
61.997862	2742.779048	20.544115
62.131384	2752.799355	20.549133
62.107465	2752.501444	20.554151
62.254262	2745.440312	20.559168
61.708505	2760.654835	20.564186
62.324706	2773.336172	20.569203
62.373692	2774.724142	20.574221
62.301612	2782.150650	20.579239
62.286069	2780.488051	20.584256
62.276742	2790.944561	20.589274
62.655327	2813.484296	20.594291
62.769110	2802.204037	20.599309
62.685602	2821.042412	20.604327
63.386945	2811.770840	20.609344
63.050331	2815.118483	20.614362
63.209866	2809.655123	20.619379
63.319141	2812.225190	20.624397
63.222932	2810.742837	20.629415
63.383174	2812.026997	20.634432
63.441936	2815.354974	20.639450
63.313815	2810.217871	20.644467
63.627514	2804.247965	20.649485
63.421097	2817.714445	20.654503
63.764052	2803.152411	20.659520
63.580015	2814.936155	20.664538
63.611754	2809.913180	20.669555
63.616803	2811.828855	20.674573
63.607189	2825.591149	20.679591
64.030159	2825.555199	20.684608
63.779532	2835.493376	20.689626
63.775604	2830.590849	20.694643
63.978795	2825.826922	20.699661
64.026210	2838.211378	20.704679
64.450413	2827.216008	20.709696
63.922377	2838.703091	20.714714
64.040600	2851.964390	20.719731
64.431277	2852.839237	20.724749
64.528456	2858.422953	20.729767
65.111433	2854.614315	20.734784
64.863957	2858.341310	20.739802
64.531630	2872.897088	20.744819
64.663284	2849.856220	20.749837
64.783657	2863.849810	20.754855
64.813999	2856.795666	20.759872
65.067566	2863.768819	20.764890
64.844252	2869.972003	20.769907
65.070195	2859.452654	20.774925
65.040852	2859.874888	20.779943
65.029657	2853.059881	20.784960
65.255745	2866.091569	20.789978
65.106904	2877.190054	20.794995
65.849947	2881.647032	20.800013
65.561973	2887.386130	20.805031
65.695519	2888.121982	20.810048
65.646322	2884.804786	20.815066
65.408903	2883.980764	20.820083
65.923185	2879.607518	20.825101
65.786065	2889.537603	20.830119
65.539386	2882.005630	20.835136
65.557930	2879.586247	20.840154
65.479826	2887.044114	20.845171
65.719161	2894.523542	20.850189
65.909572	2919.177486	20.855207
65.738243	2915.212782	20.860224
66.069814	2921.733724	20.865242
65.623766	2924.011734	20.870259
66.079216	2925.343575	20.875277
66.354702	2947.286794	20.880295
66.740891	2943.803551	20.885312
66.659713	2933.583707	20.890330
66.745474	2939.398856	20.895347
66.854543	2934.944922	20.900365
66.578706	2935.056333	20.905383
66.720831	2927.739998	20.910400
66.961817	2937.506459	20.915418
66.690892	2935.278593	20.920435
67.314001	2949.645070	20.925453
67.194983	2961.979965	20.930471
67.406034	2948.184437	20.935488
67.577305	2949.993927	20.940506
67.809886	2948.726114	20.945523
67.719077	2934.591915	20.950541
67.511394	2915.191880	20.955559
67.460712	2915.240103	20.960576
67.677843	2922.066161	20.965594
67.490707	2939.655727	20.970611
67.757914	2939.687640	20.975629
67.938044	2946.739497	20.980647
67.851873	2954.294394	20.985664
68.179616	2949.233484	20.990682
68.122240	2949.054478	20.995699
68.008813	2951.959778	21.000717
67.925242	2961.317703	21.005735
67.909749	2952.081040	21.010752
67.931246	2950.612292	21.015770
67.831022	2956.325902	21.020787
67.969488	2966.201444	21.025805
67.946297	2976.763515	21.030823
68.084649	2980.271673	21.035840
68.458149	2989.000571	21.040858
68.213740	2986.317550	21.045875
68.507452	2979.375729	21.050893
68.301753	3003.871257	21.055911
68.634549	3015.404404	21.060928
68.836286	3017.478934	21.065946
68.894348	3020.434646	21.070963
68.998842	3022.915779	21.075981
68.730222	3014.637793	21.080999
68.958010	3008.670982	21.086016
69.327382	3021.103954	21.091034
69.310937	3038.515827	21.096051
69.339493	3028.425420	21.101069
69.510671	3032.452552	21.106087
69.780824	3033.928009	21.111104
69.885613	3028.464171	21.116122
69.554698	3032.091614	21.121139
69.647338	3031.155174	21.126157
69.547788	3031.858687	21.131175
70.003170	3029.321824	21.136192
69.881119	3033.963526	21.141210
69.782560	3040.983528	21.146227
70.277731	3031.923840	21.151245
70.121703	3053.427119	21.156263
70.246790	3054.222249	21.161280
70.361636	3056.494205	21.166298
70.075328	3066.078992	21.171315
70.630994	3062.998409	21.176333
70.398201	3052.762597	21.181351
70.625536	3059.609470	21.186368
70.681139	3065.972146	21.191386
70.524769	3065.498879	21.196403
70.889390	3057.057968	21.201421
70.960183	3057.635307	21.206439
70.355371	3063.852397	21.211456
70.928115	3081.003580	21.216474
71.119139	3091.815754	21.221491
71.227579	3089.436600	21.226509
71.033972	3084.279913	21.231527
71.020030	3096.462518	21.236544
71.300188	3094.270728	21.241562
71.031057	3087.877751	21.246579
71.508932	3101.201876	21.251597
71.556463	3122.826333	21.256615
71.272833	3118.939580	21.261632
71.850337	3119.948921	21.266650
71.889526	3123.742385	21.271667
71.674695	3117.715999	21.276685
71.572458	3122.807980	21.281703
71.337284	3124.792916	21.286720
71.958361	3133.968762	21.291738
71.885336	3146.010781	21.296755
72.416099	3147.008163	21.301773
72.580568	3142.219831	21.306791
72.745004	3138.757047	21.311808
72.681321	3143.186389	21.316826
72.454798	3141.154298	21.321843
72.498640	3145.395801	21.326861
72.628169	3143.611163	21.331879
72.791240	3128.337239	21.336896
73.126981	3135.741801	21.341914
72.892906	3143.077144	21.346931
72.679718	3135.517466	21.351949
73.198704	3138.248617	21.356967
73.251508	3147.418378	21.361984
73.304737	3132.492508	21.367002
72.673064	3136.797602	21.372019
72.787293	3139.688941	21.377037
73.299009	3158.699832	21.382055
73.188288	3165.317584	21.387072
73.407535	3172.300484	21.392090
73.556734	3167.515455	21.397107
73.426504	3168.114599	21.402125
73.394665	3170.560411	21.407143
73.619818	3176.093176	21.412160
73.727719	3181.074865	21.417178
73.556681	3201.384807	21.422195
73.922566	3190.240556	21.427213
73.859171	3188.648416	21.432231
74.141624	3198.779832	21.437248
74.277215	3200.415331	21.442266
74.259496	3194.231546	21.447283
74.333686	3199.716826	21.452301
74.505528	3207.530382	21.457319
74.714694	3222.450145	21.462336
74.573301	3216.987157	21.467354
74.676074	3229.102157	21.472371
74.492711	3225.327545	21.477389
74.953409	3214.117217	21.482407
74.804886	3225.521007	21.487424
75.113256	3216.647980	21.492442
74.999217	3213.294579	21.497459
75.152957	3212.002373	21.502477
75.196751	3225.092045	21.507495
75.098935	3216.144015	21.512512
74.982604	3231.897468	21.517530
75.239879	3253.855942	21.522547
75.058081	3253.294748	21.527565
75.518129	3245.464719	21.532583
75.299425	3254.552639	21.537600
75.460987	3267.415413	21.542618
75.269253	3278.238997	21.547635
75.459929	3278.896926	21.552653
75.463039	3282.633795	21.557671
75.532158	3301.386117	21.562688
76.133045	3313.735794	21.567706
76.486838	3302.095049	21.572723
76.504813	3300.539057	21.577741
76.736735	3296.141490	21.582759
76.568456	3304.130192	21.587776
76.487128	3293.651875	21.592794
76.636925	3302.643499	21.597811
76.583808	3296.963540	21.602829
76.996125	3286.473734	21.607847
76.987655	3289.728280	21.612864
77.398688	3278.792641	21.617882
77.448396	3281.328142	21.622899
77.423793	3289.082864	21.627917
77.489082	3293.856676	21.632935
77.503239	3286.918788	21.637952
77.648188	3285.548504	21.642970
77.338595	3289.074060	21.647987
77.424019	3280.411060	21.653005
77.696334	3279.587824	21.658023
77.134783	3290.419378	21.663040
77.418552	3284.844381	21.668058
77.525319	3286.282296	21.673075
77.593215	3289.818309	21.678093
77.736797	3282.383065	21.683111
77.327742	3278.500068	21.688128
77.549819	3295.242913	21.693146
77.763348	3316.481559	21.698163
77.715700	3320.064623	21.703181
77.875941	3323.126341	21.708199
77.624627	3326.258034	21.713216
78.069941	3346.505689	21.718234
78.106432	3338.594425	21.723251
77.980893	3352.182252	21.728269
78.424462	3358.164412	21.733287
78.239986	3369.313625	21.738304
78.575846	3379.744989	21.743322
78.616211	3389.896454	21.748339
78.895748	3375.899864	21.753357
78.922244	3369.252413	21.758375
78.822801	3394.036110	21.763392
79.144962	3405.121709	21.768410
79.478506	3405.344628	21.773427
79.384242	3406.645304	21.778445
79.623684	3399.155583	21.783463
79.478356	3395.181341	21.788480
79.868851	3399.896724	21.793498
79.882851	3390.006120	21.798515
79.580335	3389.823129	21.803533
80.174302	3390.182932	21.808551
79.808462	3400.108618	21.813568
79.892673	3395.678739	21.818586
79.994787	3393.001378	21.823603
80.145129	3390.003850	21.828621
80.254392	3403.298203	21.833639
80.387259	3420.556308	21.838656
80.620477	3418.031685	21.843674
80.476013	3412.586458	21.848691
80.763428	3414.100438	21.853709
80.717095	3417.125838	21.858727
80.728489	3425.861670	21.863744
80.488768	3407.593456	21.868762
80.658187	3417.652356	21.873779
80.889236	3414.904868	21.878797
81.064394	3407.495449	21.883815
80.648862	3414.530201	21.888832
81.137148	3423.768715	21.893850
81.472589	3434.206484	21.898867
81.558610	3432.299084	21.903885
81.434498	3435.106635	21.908903
81.375386	3429.255180	21.913920
81.387983	3434.412144	21.918938
81.547101	3427.532915	21.923955
81.534432	3443.052922	21.928973
81.849214	3440.757333	21.933991
81.891702	3451.680915	21.939008
81.837871	3456.653985	21.944026
81.801449	3475.933792	21.949043
82.050608	3465.213351	21.954061
82.480596	3453.976824	21.959079
82.286760	3466.536290	21.964096
82.406392	3460.931661	21.969114
82.402785	3454.583237	21.974131
82.088967	3467.049933	21.979149
82.462142	3484.295959	21.984167
82.475604	3491.335055	21.989184
82.497630	3485.237891	21.994202
82.287010	3479.033505	21.999219
82.247207	3492.428156	22.004237
82.528195	3493.154636	22.009255
82.925040	3521.286401	22.014272
83.237446	3525.306861	22.019290
83.710538	3504.448338	22.024307
83.369697	3516.850642	22.029325
83.550297	3498.805383	22.034343
83.726471	3511.877753	22.039360
83.798824	3512.493435	22.044378
83.723138	3504.628969	22.049395
83.534211	3507.674405	22.054413
84.000363	3525.890534	22.059431
84.019420	3534.185795	22.064448
84.197860	3526.913177	22.069466
84.515275	3533.239476	22.074483
84.365344	3544.370508	22.079501
84.565943	3534.316697	22.084519
84.605426	3537.829509	22.089536
84.423039	3542.611646	22.094554
84.562648	3529.556927	22.099571
84.644285	3539.560334	22.104589
84.792460	3529.322278	22.109607
84.700033	3530.866752	22.114624
84.647120	3530.777551	22.119642
84.863555	3531.034784	22.124659
85.043497	3540.633763	22.129677
85.007693	3534.883927	22.134695
85.247290	3562.112234	22.139712
85.053303	3557.984575	22.144730
85.676291	3560.194687	22.149747
85.386256	3579.376767	22.154765
85.493116	3563.449504	22.159783
85.240222	3565.607893	22.164800
85.009368	3575.695636	22.169818
85.592021	3584.133227	22.174835
85.504490	3587.193814	22.179853
85.795594	3599.565777	22.184871
85.736195	3590.794645	22.189888
85.978806	3607.396247	22.194906
86.215483	3617.670146	22.199923
86.208370	3619.825725	22.204941
86.321062	3620.591437	22.209959
86.327869	3621.439212	22.214976
86.415916	3611.201982	22.219994
86.668274	3607.133232	22.225011
86.783463	3625.337786	22.230029
87.070369	3620.140103	22.235047
86.967083	3635.581969	22.240064
86.940774	3639.219848	22.245082
87.250511	3642.349052	22.250099
87.170517	3645.477302	22.255117
87.164313	3633.170996	22.260135
87.313291	3640.546820	22.265152
87.431755	3634.482482	22.270170
87.237399	3626.282053	22.275187
87.227076	3660.106121	22.280205
87.411180	3660.849799	22.285223
87.738675	3668.347712	22.290240
87.912874	3673.250495	22.295258
88.185062	3664.348941	22.300275
88.041238	3675.475907	22.305293
88.562429	3674.300112	22.310311
88.331393	3669.181303	22.315328
88.077290	3657.687985	22.320346
88.249138	3666.313187	22.325363
88.281493	3697.378719	22.330381
88.271031	3689.290390	22.335399
88.503652	3697.898481	22.340416
88.594305	3706.530429	22.345434
88.860273	3701.151926	22.350451
88.541594	3698.467666	22.355469
88.621163	3707.300658	22.360487
89.014947	3724.935673	22.365504
88.779999	3742.017117	22.370522
89.242012	3729.192029	22.375539
89.314897	3725.973771	22.380557
89.263168	3717.067442	22.385575
89.543784	3731.777464	22.390592
89.388217	3758.780861	22.395610
89.976822	3749.289178	22.400627
89.931193	3749.648773	22.405645
89.938982	3740.711337	22.410663
90.267206	3741.528449	22.415680
90.407673	3738.667919	22.420698
90.357177	3731.085003	22.425715
90.136308	3741.829471	22.430733
90.144325	3740.047128	22.435751
90.458875	3739.562954	22.440768
90.278941	3739.503402	22.445786
90.596751	3725.784427	22.450803
90.544017	3762.437381	22.455821
90.221581	3774.854958	22.460839
90.798102	3771.070792	22.465856
91.017259	3767.056306	22.470874
90.699376	3766.830965	22.475891
90.934058	3784.128557	22.480909
91.422035	3787.657475	22.485927
91.636945	3794.226805	22.490944
91.549442	3804.419749	22.495962
91.414511	3802.387789	22.500979
91.536974	3795.853433	22.505997
91.668271	3803.698400	22.511015
91.793676	3797.013950	22.516032
91.805455	3797.668786	22.521050
91.742310	3805.101393	22.526067
91.901475	3820.025663	22.531085
91.988060	3831.472545	22.536103
92.225869	3832.228224	22.541120
92.037254	3838.297317	22.546138
92.600569	3820.227029	22.551155
92.399814	3824.426063	22.556173
92.352905	3844.753343	22.561191
92.747969	3840.836938	22.566208
92.629639	3853.220458	22.571226
92.928550	3853.304225	22.576243
93.097836	3846.990066	22.581261
93.321403	3842.201203	22.586279
93.169456	3840.099608	22.591296
92.974192	3844.914281	22.596314
93.471998	3857.014104	22.601331
93.283703	3877.117543	22.606349
93.247342	3879.387833	22.611367
93.527599	3872.952570	22.616384
93.385936	3876.172159	22.621402
93.588391	3884.863292	22.626419
93.929461	3903.244236	22.631437
93.743731	3912.279059	22.636455
93.978926	3909.498909	22.641472
94.088968	3909.341834	22.646490
94.112508	3916.749935	22.651507
94.235400	3927.599148	22.656525
94.257654	3938.550432	22.661543
94.592876	3940.104992	22.666560
94.324505	3947.344016	22.671578
94.605189	3938.508226	22.676595
94.458796	3945.062910	22.681613
94.447416	3959.107213	22.686631
95.346795	3961.123289	22.691648
95.206111	3964.611243	22.696666
95.428847	3967.308032	22.701683
95.765092	3966.041516	22.706701
95.736367	3958.177721	22.711719
95.948180	3960.513711	22.716736
95.402860	3969.796963	22.721754
95.598115	3967.221438	22.726771
95.562736	3955.081118	22.731789
95.694184	3954.722865	22.736807
95.685925	3968.186731	22.741824
95.517805	3966.972845	22.746842
95.741014	3992.568762	22.751859
95.957947	4000.868584	22.756877
95.831703	4007.688081	22.761895
96.243254	4014.226587	22.766912
96.296324	4040.556221	22.771930
96.593911	4016.966115	22.776947
96.419714	4025.116403	22.781965
96.224356	4050.171329	22.786983
96.827022	4057.067652	22.792000
96.834757	4061.137809	22.797018
96.953007	4061.950264	22.802035
96.821110	4069.354593	22.807053
97.106431	4082.541301	22.812071
97.805745	4078.952526	22.817088
97.668785	4087.964824	22.822106
97.732704	4077.434811	22.827123
98.029588	4077.571672	22.832141
97.990030	4079.738187	22.837159
98.072987	4081.050974	22.842176
97.791681	4091.923783	22.847194
98.026813	4076.003935	22.852211
98.237352	4085.380475	22.857229
98.300634	4095.760511	22.862247
98.556341	4103.398060	22.867264
98.455859	4104.051380	22.872282
98.395502	4108.212723	22.877299
98.478654	4105.720662	22.882317
98.469995	4104.313089	22.887335
98.829635	4108.455822	22.892352
98.689696	4129.001212	22.897370
98.815306	4122.334307	22.902387
99.078403	4124.838623	22.907405
99.102831	4134.731785	22.912423
99.560569	4128.745056	22.917440
99.635127	4145.976593	22.922458
99.777473	4165.332442	22.927475
99.825577	4156.905837	22.932493
99.476161	4152.891498	22.937511
100.139966	4160.834882	22.942528
100.153625	4155.291610	22.947546
100.028360	4157.910106	22.952563
100.484486	4157.721828	22.957581
100.028733	4148.555625	22.962599
100.387628	4152.396123	22.967616
100.533052	4171.556978	22.972634
100.490724	4174.411386	22.977651
100.993731	4174.198431	22.982669
100.942014	4186.809406	22.987687
101.335038	4176.441094	22.992704
101.218876	4182.180229	22.997722
100.899102	4182.395363	23.002739
101.350324	4174.321836	23.007757
100.932365	4174.109874	23.012775
101.361705	4170.149140	23.017792
101.189732	4180.029112	23.022810
101.449405	4193.152829	23.027827
101.463539	4195.824677	23.032845
101.424482	4224.358889	23.037863
101.713925	4200.515906	23.042880
101.692651	4203.860556	23.047898
101.830691	4227.031486	23.052915
102.039726	4230.874719	23.057933
102.048802	4238.657421	23.062951
101.796655	4244.591889	23.067968
102.008846	4241.739496	23.072986
102.494311	4261.728950	23.078003
102.516667	4264.869153	23.083021
102.430949	4273.467565	23.088039
102.509683	4278.948145	23.093056
102.715698	4281.463495	23.098074
102.925017	4293.495576	23.103091
102.957879	4294.758783	23.108109
103.089140	4303.310729	23.113127
103.285333	4300.444826	23.118144
103.614096	4306.866422	23.123162
103.509554	4310.953622	23.128179
103.758167	4317.703833	23.133197
103.592070	4330.803920	23.138215
103.879413	4310.786070	23.143232
104.176515	4313.001717	23.148250
104.110272	4313.313942	23.153267
104.429377	4310.915148	23.158285
104.475059	4323.073508	23.163303
104.695623	4331.793397	23.168320
104.636018	4340.716284	23.173338
104.565717	4335.209263	23.178355
105.037686	4340.714262	23.183373
104.756849	4347.507087	23.188391
105.045409	4345.273971	23.193408
105.177201	4329.088253	23.198426
105.235772	4337.036455	23.203443
105.544270	4331.723154	23.208461
105.184973	4331.014075	23.213479
105.380638	4353.047280	23.218496
105.634832	4352.782127	23.223514
105.654538	4358.660694	23.228531
105.985281	4360.015243	23.233549
105.901095	4366.608252	23.238567
105.743018	4354.628845	23.243584
106.372907	4363.573649	23.248602
106.633846	4385.802029	23.253619
106.458962	4382.532840	23.258637
106.685995	4377.624733	23.263655
106.858660	4392.062656	23.268672
107.020251	4391.045841	23.273690
106.600751	4393.306284	23.278707
106.997766	4378.186581	23.283725
107.245551	4388.114260	23.288743
107.203089	4382.391196	23.293760
107.246856	4385.005816	23.298778
107.004603	4380.566606	23.303795
107.062722	4387.764877	23.308813
106.958828	4408.419645	23.313831
107.330006	4416.810351	23.318848
107.420525	4408.427784	23.323866
107.482282	4435.964580	23.328883
107.848675	4446.501467	23.333901
107.841027	4453.773631	23.338919
107.853139	4444.190952	23.343936
107.832300	4456.770269	23.348954
107.865949	4488.438376	23.353971
108.492403	4471.801858	23.358989
108.451512	4471.835867	23.364007
108.710755	4475.576766	23.369024
108.817349	4467.254507	23.374042
108.604570	4472.408502	23.379059
109.199039	4485.566914	23.384077
109.273758	4499.211632	23.389095
109.497783	4501.260633	23.394112
109.499021	4496.027575	23.399130
109.432484	4496.142598	23.404147
109.934759	4495.483284	23.409165
109.588646	4496.167363	23.414183
109.737669	4496.963339	23.419200
109.630826	4502.458126	23.424218
109.805037	4502.430607	23.429235
110.064496	4515.261703	23.434253
109.948675	4526.219680	23.439271
110.080446	4536.558769	23.444288
110.175817	4519.711514	23.449306
110.373904	4531.699964	23.454323
110.278147	4545.449667	23.459341
110.400498	4551.551910	23.464359
110.649305	4554.034642	23.469376
111.012437	4550.212713	23.474394
110.638328	4564.429315	23.479411
111.139184	4577.734776	23.484429
111.456595	4580.156567	23.489447
111.330734	4587.017200	23.494464
111.543161	4574.090528	23.499482
111.419842	4592.576976	23.504499
111.905555	4595.637927	23.509517
112.111895	4603.903601	23.514535
112.158609	4612.427164	23.519552
112.181693	4602.657131	23.524570
112.238885	4611.422677	23.529587
112.306164	4601.393753	23.534605
112.369795	4600.244678	23.539623
112.053665	4600.014307	23.544640
112.912302	4616.667176	23.549658
112.588886	4631.782995	23.554675
112.515041	4629.086857	23.559693
112.747817	4629.054386	23.564711
112.684008	4645.779781	23.569728
113.095683	4660.650536	23.574746
113.345812	4656.986632	23.579763
113.427047	4658.207622	23.584781
113.691145	4662.741119	23.589799
113.314632	4656.813292	23.594816
113.936409	4677.294570	23.599834
113.736521	4693.066850	23.604851
114.101591	4698.288441	23.609869
114.183869	4693.780162	23.614887
114.388386	4700.024014	23.619904
114.792823	4690.123587	23.624922
114.455163	4697.452362	23.629939
114.742953	4700.720852	23.634957
114.713874	4698.336617	23.639975
114.872359	4705.388128	23.644992
114.916383	4709.690662	23.650010
115.071555	4707.561038	23.655027
115.084172	4699.448684	23.660045
115.558984	4701.647624	23.665063
115.360255	4708.480978	23.670080
115.817066	4699.656211	23.675098
115.295894	4714.544533	23.680115
115.496899	4716.856438	23.685133
115.936999	4734.948365	23.690151
115.596622	4745.114411	23.695168
116.015489	4732.662192	23.700186
115.781875	4733.784414	23.705203
116.316165	4754.065668	23.710221
116.469429	4759.934917	23.715239
116.501751	4756.434941	23.720256
116.974390	4768.316000	23.725274
116.550241	4763.858307	23.730291
116.676973	4751.202358	23.735309
117.127232	4762.365016	23.740327
116.746488	4760.282595	23.745344
116.923627	4760.937316	23.750362
117.299971	4786.747048	23.755379
117.225614	4788.972564	23.760397
117.446681	4795.999208	23.765415
117.746554	4788.627587	23.770432
118.083908	4789.416871	23.775450
117.816289	4802.799895	23.780467
117.823032	4812.364496	23.785485
118.243654	4821.040185	23.790503
117.979554	4821.590639	23.795520
118.396034	4808.934802	23.800538
118.342811	4818.555382	23.805555
118.202832	4835.149461	23.810573
118.447084	4845.028800	23.815591
118.467985	4852.132247	23.820608
118.698866	4853.865573	23.825626
118.383707	4871.136714	23.830643
118.819188	4866.237716	23.835661
119.296088	4882.843705	23.840679
119.290039	4909.874785	23.845696
119.487454	4905.185991	23.850714
119.398705	4907.353268	23.855731
119.314392	4907.586200	23.860749
119.774808	4921.402615	23.865767
119.737597	4935.964310	23.870784
119.825632	4935.982923	23.875802
120.377224	4939.484669	23.880819
120.347482	4969.380228	23.885837
120.425808	4975.971840	23.890855
120.416198	4980.471122	23.895872
120.815945	4969.398758	23.900890
120.633250	4973.791587	23.905907
121.190671	4989.849302	23.910925
120.886816	4987.112360	23.915943
121.176807	4996.319617	23.920960
121.377043	4998.370253	23.925978
121.517271	4992.080514	23.930995
121.565058	5014.144208	23.936013
121.775123	5030.508199	23.941031
121.829119	5026.567537	23.946048
121.744096	5028.032581	23.951066
121.965836	5027.026656	23.956083
121.905019	5038.097566	23.961101
122.106638	5057.046271	23.966119
122.508706	5055.548697	23.971136
122.924229	5047.072713	23.976154
122.587910	5046.761017	23.981171
122.458644	5057.013258	23.986189
123.075800	5076.727256	23.991207
123.004507	5085.317825	23.996224
123.168959	5079.511492	24.001242
123.569667	5077.525516	24.006259
123.324362	5082.781157	24.011277
123.350431	5087.800211	24.016295
123.619759	5113.160408	24.021312
123.953939	5108.084356	24.026330
123.771452	5105.293872	24.031347
124.057845	5114.374223	24.036365
124.377487	5104.676145	24.041383
124.373350	5119.554622	24.046400
124.422169	5138.779090	24.051418
124.676108	5141.337848	24.056435
124.845005	5128.478940	24.061453
124.928575	5138.299969	24.066471
124.746659	5142.143847	24.071488
124.804423	5124.195754	24.076506
125.105637	5133.165389	24.081523
124.903673	5142.807595	24.086541
125.249132	5143.468382	24.091559
125.429705	5154.412867	24.096576
125.342692	5158.891128	24.101594
125.682592	5166.219987	24.106611
125.720423	5181.986160	24.111629
125.762486	5178.412033	24.116647
125.973569	5187.496602	24.121664
126.223200	5190.041905	24.126682
126.396670	5202.494826	24.131699
125.997895	5222.114250	24.136717
126.318088	5214.619376	24.141735
126.379986	5221.209081	24.146752
126.763334	5242.985740	24.151770
126.594406	5238.159722	24.156787
126.742503	5249.638038	24.161805
127.195204	5263.046542	24.166823
127.382274	5279.312222	24.171840
127.842444	5277.896375	24.176858
127.529948	5275.466746	24.181875
127.615204	5288.159923	24.186893
128.040786	5289.198069	24.191911
127.633992	5305.003971	24.196928
127.753701	5319.597581	24.201946
128.462707	5313.486596	24.206963
128.097177	5309.380119	24.211981
128.480694	5321.330663	24.216999
128.687880	5335.846049	24.222016
128.866931	5324.684298	24.227034
129.236280	5331.133870	24.232051
129.051392	5335.484244	24.237069
129.402357	5338.507761	24.242087
129.826296	5356.724748	24.247104
129.890686	5358.743936	24.252122
130.308924	5351.925782	24.257139
130.137387	5357.591811	24.262157
130.239815	5356.877656	24.267175
130.089393	5352.572615	24.272192
130.133074	5342.879433	24.277210
130.195069	5346.771651	24.282227
130.155786	5360.480451	24.287245
130.355204	5352.935381	24.292263
130.560238	5380.928566	24.297280
130.731036	5377.648116	24.302298
130.594181	5377.844062	24.307315
130.751188	5394.180978	24.312333
131.282611	5397.014830	24.317351
130.965237	5407.072767	24.322368
131.206539	5414.908639	24.327386
131.667975	5426.113634	24.332403
131.194471	5452.170806	24.337421
131.641553	5441.395048	24.342439
131.148194	5458.914414	24.347456
131.526555	5471.187615	24.352474
131.854130	5472.791242	24.357491
131.598651	5484.026930	24.362509
132.201802	5512.247120	24.367527
132.182423	5512.075979	24.372544
132.611186	5525.230761	24.377562
133.085968	5528.668160	24.382579
133.055767	5536.595811	24.387597
133.749908	5532.294889	24.392615
133.297329	5527.437687	24.397632
133.610505	5516.230801	24.402650
134.146604	5526.197405	24.407667
133.636165	5526.333807	24.412685
133.991182	5527.861637	24.417703
134.043411	5518.782360	24.422720
133.972907	5517.553008	24.427738
134.286776	5530.035754	24.432755
134.390555	5542.918620	24.437773
134.579047	5556.723830	24.442791
134.620945	5547.019004	24.447808
134.957087	5547.143098	24.452826
134.881114	5553.242278	24.457843
134.543601	5548.477488	24.462861
135.094673	5567.683282	24.467879
135.335712	5581.511332	24.472896
135.580351	5585.418318	24.477914
135.579816	5584.466410	24.482931
135.673222	5589.286287	24.487949
135.647875	5585.870073	24.492967
135.980010	5589.514542	24.497984
135.694141	5603.215080	24.503002
136.147897	5604.211187	24.508019
135.658250	5625.661703	24.513037
136.033000	5625.227383	24.518055
136.104150	5637.275852	24.523072
136.274154	5658.347700	24.528090
136.542352	5654.810124	24.533107
136.635095	5673.723623	24.538125
136.939538	5688.208304	24.543143
137.330868	5692.182035	24.548160
137.847910	5698.004525	24.553178
137.481210	5695.000246	24.558195
137.794633	5694.283107	24.563213
138.045233	5700.494941	24.568231
138.018755	5718.262297	24.573248
138.000354	5721.557578	24.578266
138.455555	5719.095530	24.583283
138.455950	5727.587193	24.588301
138.800736	5718.615386	24.593319
138.876624	5730.830095	24.598336
138.902328	5740.875263	24.603354
139.168002	5735.262228	24.608371
139.287125	5750.118969	24.613389
139.179801	5743.386700	24.618407
139.084336	5751.084660	24.623424
139.348295	5762.116199	24.628442
139.616179	5770.393193	24.633459
139.464169	5777.419317	24.638477
139.635824	5779.077484	24.643495
139.846330	5799.118678	24.648512
140.100865	5807.991677	24.653530
140.268060	5799.809505	24.658547
140.139629	5828.726422	24.663565
140.508939	5832.879443	24.668583
140.916773	5833.566182	24.673600
140.650589	5850.466872	24.678618
141.066321	5848.126303	24.683635
141.002485	5866.314229	24.688653
141.020226	5872.625639	24.693671
141.591159	5866.399837	24.698688
141.605518	5889.005400	24.703706
141.980278	5882.032764	24.708723
141.977695	5900.781947	24.713741
141.897734	5907.172516	24.718759
142.148152	5893.079657	24.723776
142.016719	5903.240670	24.728794
142.280563	5909.027505	24.733811
142.331024	5924.177686	24.738829
142.484775	5925.515552	24.743847
142.956989	5919.639552	24.748864
142.861974	5943.411459	24.753882
143.317850	5944.415902	24.758899
143.352798	5947.479156	24.763917
143.513489	5949.795545	24.768935
143.708552	5952.224383	24.773952
143.493203	5962.641066	24.778970
143.781864	5970.731242	24.783987
144.052969	5976.851991	24.789005
143.847313	5980.244417	24.794023
144.212657	5985.470731	24.799040
144.095880	5998.002956	24.804058
144.561487	5992.886400	24.809075
144.742118	6005.054090	24.814093
144.728842	6017.659794	24.819111
145.194733	6011.319776	24.824128
144.905451	6032.083312	24.829146
145.219644	6038.841156	24.834163
145.554007	6044.565595	24.839181
145.492362	6047.303044	24.844199
145.820746	6047.085068	24.849216
145.671311	6055.469361	24.854234
145.829721	6058.530349	24.859251
146.005139	6057.528865	24.864269
146.045839	6083.322172	24.869287
146.276659	6082.173716	24.874304
146.476573	6087.791233	24.879322
146.553500	6110.566331	24.884339
146.471346	6110.539828	24.889357
146.657515	6121.341524	24.894375
147.051556	6145.344789	24.899392
147.150386	6156.002647	24.904410
147.237502	6151.370297	24.909427
147.673767	6166.305367	24.914445
147.590369	6183.166762	24.919463
147.727239	6173.537998	24.924480
147.580207	6188.015836	24.929498
148.165922	6206.192908	24.934515
148.544115	6206.647911	24.939533
148.793584	6211.246100	24.944551
149.025638	6202.009529	24.949568
149.159431	6211.729217	24.954586
149.311365	6232.589435	24.959603
149.539463	6228.548827	24.964621
149.724168	6241.255090	24.969639
149.864278	6228.635511	24.974656
149.491413	6229.983238	24.979674
149.794946	6231.198730	24.984691
149.946261	6239.589343	24.989709
150.116105	6241.134848	24.994727
150.289175	6251.359965	24.999744
150.579944	6262.020045	25.004762
150.655444	6262.061996	25.009779
150.882908	6260.261220	25.014797
150.779866	6260.915443	25.019815
150.841139	6265.594358	25.024832
150.798153	6280.757566	25.029850
150.982137	6283.226088	25.034867
151.188917	6296.486321	25.039885
151.078900	6312.016599	25.044903
151.415887	6326.713853	25.049920
151.588205	6328.023486	25.054938
152.003237	6343.065400	25.059955
152.184173	6348.238040	25.064973
152.065959	6348.734904	25.069991
152.637221	6340.949546	25.075008
152.648005	6356.526061	25.080026
152.738178	6356.045028	25.085043
152.927395	6374.051549	25.090061
152.986675	6392.605634	25.095079
152.876599	6374.065627	25.100096
153.048933	6395.307007	25.105114
153.536589	6406.621387	25.110131
153.689232	6398.001076	25.115149
153.506688	6408.018078	25.120167
154.091507	6418.006737	25.125184
153.967103	6437.457516	25.130202
154.122492	6438.404538	25.135219
154.396151	6437.328520	25.140237
154.282728	6448.919442	25.145255
154.706459	6460.048325	25.150272
154.640840	6461.618582	25.155290
154.856657	6474.441175	25.160307
154.741517	6479.694280	25.165325
155.259651	6491.925896	25.170343
155.628444	6491.484665	25.175360
155.704220	6491.111537	25.180378
155.803621	6493.730312	25.185395
156.461557	6507.555664	25.190413
156.481715	6515.793261	25.195431
156.141284	6512.510416	25.200448
156.235756	6507.753102	25.205466
156.414554	6524.473098	25.210483
156.606027	6538.907929	25.215501
156.577417	6539.471111	25.220519
156.851282	6543.198282	25.225536
156.871493	6565.881031	25.230554
156.960892	6571.683941	25.235571
157.390324	6587.754609	25.240589
157.528669	6604.474286	25.245607
158.018297	6599.253942	25.250624
157.755582	6611.497325	25.255642
157.970640	6620.367464	25.260659
158.589534	6633.503186	25.265677
158.579859	6636.183323	25.270695
158.743669	6626.612834	25.275712
158.729060	6645.388914	25.280730
158.933667	6663.232563	25.285747
159.412917	6657.620141	25.290765
158.909195	6670.607460	25.295783
159.523570	6675.749544	25.300800
159.669169	6689.782567	25.305818
159.464419	6693.847171	25.310835
159.925213	6699.441492	25.315853
160.371191	6720.781433	25.320871
160.433407	6726.590467	25.325888
160.284016	6730.260032	25.330906
160.612859	6734.019905	25.335923
160.900058	6729.525225	25.340941
160.955074	6747.840230	25.345959
160.920797	6754.274785	25.350976
161.468143	6756.753437	25.355994
161.197763	6752.828924	25.361011
161.530710	6766.015153	25.366029
161.369169	6781.707981	25.371047
162.038442	6782.059781	25.376064
162.100501	6791.460119	25.381082
162.175993	6800.142355	25.386099
162.742119	6809.608268	25.391117
162.635756	6805.866131	25.396135
163.025664	6813.363130	25.401152
162.966821	6814.718086	25.406170
162.973450	6807.699943	25.411187
163.235917	6798.702929	25.416205
163.030428	6825.750181	25.421223
163.140783	6834.764538	25.426240
163.469798	6837.953428	25.431258
163.379104	6857.077831	25.436275
163.769463	6862.617694	25.441293
164.015420	6871.934142	25.446311
163.686978	6876.162565	25.451328
163.747977	6894.991817	25.456346
163.888741	6899.914532	25.461363
164.253652	6915.440965	25.466381
163.927671	6939.244661	25.471399
164.430436	6950.542763	25.476416
165.257563	6960.759508	25.481434
165.130945	6973.974591	25.486451
165.658306	6981.853768	25.491469
165.547356	6996.070428	25.496487
165.860723	6986.580544	25.501504
166.095877	6995.189253	25.506522
166.189664	7020.529563	25.511539
166.716939	7005.716597	25.516557
166.388044	7022.435163	25.521575
166.499710	7029.467894	25.526592
166.582552	7043.137507	25.531610
166.863545	7049.338950	25.536627
167.360213	7057.278367	25.541645
167.308567	7076.778556	25.546663
167.587433	7067.847199	25.551680
167.919173	7070.112654	25.556698
167.987917	7087.266482	25.561715
168.218250	7095.362547	25.566733
168.261382	7109.659385	25.571751
168.002026	7108.487887	25.576768
168.478005	7120.961657	25.581786
168.769023	7141.350396	25.586803
168.979207	7138.631704	25.591821
169.072891	7145.775356	25.596839
169.173851	7164.401434	25.601856
169.585474	7166.158321	25.606874
169.685708	7174.071939	25.611891
170.003637	7170.132812	25.616909
169.942186	7179.745958	25.621927
170.155767	7189.282952	25.626944
170.364546	7197.155808	25.631962
170.395090	7208.018619	25.636979
170.469612	7216.101111	25.641997
170.319270	7233.009344	25.647015
170.544466	7239.635923	25.652032
170.894352	7245.703199	25.657050
170.611599	7265.291423	25.662067
171.470970	7271.238300	25.667085
171.680617	7291.847024	25.672103
171.878252	7293.143106	25.677120
172.043052	7302.204653	25.682138
172.036060	7331.787491	25.687156
172.483401	7317.750609	25.692173
172.571622	7332.693893	25.697191
172.889192	7338.564923	25.702208
173.157064	7342.792604	25.707226
172.871000	7353.343175	25.712244
172.996059	7358.607290	25.717261
173.163093	7376.898217	25.722279
173.409517	7386.166062	25.727296
173.520266	7385.335061	25.732314
173.431557	7401.126732	25.737332
173.665583	7424.870923	25.742349
173.967274	7426.868103	25.747367
173.790490	7444.725249	25.752384
174.228405	7456.788941	25.757402
174.462611	7465.735153	25.762420
174.626536	7474.371646	25.767437
174.718807	7491.641740	25.772455
174.929957	7490.503524	25.777472
175.067840	7507.628271	25.782490
175.501319	7515.723279	25.787508
175.730418	7504.632445	25.792525
176.331991	7517.453585	25.797543
176.391790	7536.194016	25.802560
176.651737	7534.238875	25.807578
176.327591	7527.770460	25.812596
176.780033	7531.242323	25.817613
176.923614	7539.258439	25.822631
177.032821	7554.176412	25.827648
177.272463	7561.757668	25.832666
177.143166	7578.220164	25.837684
177.208379	7579.179793	25.842701
177.543855	7587.147688	25.847719
177.725633	7600.985735	25.852736
177.839394	7614.274263	25.857754
177.922301	7633.442594	25.862772
178.300939	7626.782411	25.867789
178.337802	7631.585480	25.872807
178.461017	7647.152570	25.877824
178.750279	7660.809878	25.882842
178.773366	7688.880161	25.887860
178.699482	7684.440935	25.892877
179.236272	7710.026560	25.897895
179.106750	7731.778002	25.902912
179.530764	7736.189493	25.907930
179.478722	7759.798729	25.912948
180.035509	7775.204522	25.917965
180.380063	7791.456630	25.922983
180.214702	7791.039828	25.928000
180.731239	7808.685955	25.933018
180.880380	7831.748538	25.938036
181.165390	7822.163603	25.943053
181.619448	7823.527628	25.948071
181.641790	7838.837486	25.953088
181.911999	7837.312223	25.958106
181.896956	7845.888702	25.963124
182.097476	7846.343975	25.968141
182.201565	7865.990317	25.973159
182.498392	7879.529998	25.978176
182.767288	7877.601692	25.983194
183.018399	7882.185138	25.988212
183.090774	7897.839636	25.993229
183.623756	7899.841194	25.998247
183.782032	7898.851093	26.003264
183.716163	7893.599244	26.008282
183.881520	7903.431329	26.013300
184.096100	7929.364327	26.018317
184.218428	7937.980380	26.023335
184.039004	7935.555908	26.028352
184.182322	7940.786484	26.033370
184.461566	7952.557790	26.038388
184.500345	7958.130928	26.043405
184.638131	7969.349086	26.048423
184.612904	7988.407332	26.053440
184.838865	7996.617212	26.058458
185.204718	8024.518042	26.063476
185.187406	8026.315181	26.068493
185.538279	8046.260436	26.073511
185.731530	8062.685108	26.078528
185.948800	8078.956967	26.083546
185.896613	8092.725410	26.088564
186.222733	8118.727715	26.093581
186.554303	8124.820412	26.098599
186.782251	8127.629305	26.103616
187.127086	8146.670705	26.108634
187.093371	8157.675532	26.113652
187.681590	8160.618661	26.118669
188.024093	8164.677496	26.123687
187.959662	8171.134149	26.128704
188.456879	8182.327727	26.133722
188.551883	8190.362439	26.138740
188.484101	8193.912528	26.143757
188.596354	8185.549958	26.148775
188.778827	8208.571354	26.153792
188.967734	8212.265703	26.158810
189.235192	8216.202267	26.163828
189.460460	8233.455136	26.168845
189.687319	8243.508046	26.173863
189.667890	8250.268409	26.178880
189.784047	8258.662758	26.183898
189.689683	8275.825922	26.188916
190.215846	8270.950284	26.193933
190.390861	8299.367522	26.198951
190.311621	8313.890451	26.203968
190.954728	8317.664945	26.208986
190.954484	8331.438403	26.214004
191.012942	8346.152847	26.219021
191.090990	8357.210233	26.224039
191.590534	8366.329717	26.229056
191.880126	8377.768037	26.234074
192.004012	8389.459794	26.239092
191.986980	8411.747290	26.244109
192.395809	8413.192879	26.249127
192.237005	8436.509646	26.254144
192.773878	8441.443011	26.259162
192.865166	8452.874767	26.264180
193.265333	8461.381402	26.269197
193.658826	8468.506836	26.274215
194.161319	8490.414028	26.279232
193.922243	8491.183758	26.284250
194.296277	8486.285144	26.289268
194.521680	8500.469634	26.294285
194.475266	8499.260483	26.299303
194.513069	8513.023086	26.304320
194.689062	8523.840716	26.309338
195.073263	8541.218888	26.314356
194.883404	8541.814296	26.319373
195.074776	8554.078669	26.324391
194.858842	8583.165919	26.329408
195.742058	8591.492783	26.334426
196.130600	8609.642207	26.339444
195.859042	8621.624738	26.344461
196.209823	8618.754180	26.349479
196.735800	8637.181809	26.354496
197.232612	8629.872354	26.359514
197.427203	8637.263084	26.364532
197.441048	8644.856963	26.369549
197.664429	8660.994512	26.374567
197.873006	8673.379795	26.379584
197.814258	8669.302473	26.384602
197.718031	8671.720002	26.389620
197.856195	8699.786454	26.394637
198.328199	8694.465162	26.399655
198.831409	8717.860424	26.404672
199.034660	8725.066241	26.409690
198.628474	8743.524345	26.414708
198.910748	8743.237560	26.419725
199.323163	8743.108070	26.424743
199.379751	8770.560364	26.429760
199.494836	8766.700045	26.434778
200.024366	8791.894009	26.439796
200.275833	8803.801290	26.444813
200.175828	8795.656206	26.449831
199.977831	8807.296696	26.454848
200.275880	8825.581830	26.459866
200.807918	8841.711888	26.464884
200.775877	8851.931623	26.469901
201.130748	8861.402176	26.474919
201.520165	8872.655802	26.479936
201.457463	8888.618729	26.484954
201.722032	8892.812718	26.489972
201.683432	8908.340832	26.494989
202.507953	8924.705421	26.500007
202.215739	8932.524866	26.505024
202.323284	8946.157384	26.510042
202.804333	8942.477582	26.515060
203.031644	8967.840697	26.520077
203.125705	8976.996810	26.525095
203.183821	8982.178795	26.530112
203.615921	9011.314930	26.535130
204.159971	9017.405162	26.540148
204.301166	9022.684494	26.545165
204.531697	9030.080497	26.550183
204.751449	9039.915329	26.555200
204.890047	9039.712140	26.560218
205.053696	9055.997802	26.565236
205.095444	9072.569066	26.570253
205.359385	9065.428642	26.575271
205.506426	9092.508159	26.580288
205.856284	9104.799547	26.585306
205.857159	9097.398531	26.590324
206.419726	9117.755196	26.595341
206.420639	9129.296892	26.600359
206.272897	9133.759923	26.605376
206.624385	9150.927560	26.610394
206.862125	9150.118810	26.615412
207.044451	9172.278339	26.620429
207.205153	9191.915395	26.625447
207.440131	9201.838395	26.630464
207.720523	9226.300715	26.635482
208.109485	9228.367992	26.640500
207.956658	9252.507302	26.645517
208.358582	9263.038414	26.650535
208.722801	9282.958605	26.655552
208.670923	9299.284064	26.660570
209.064310	9295.447739	26.665588
208.727205	9324.324785	26.670605
209.287874	9325.217628	26.675623
209.548399	9350.407302	26.680640
209.822649	9355.918396	26.685658
209.938423	9374.815590	26.690676
210.037188	9397.128658	26.695693
210.531474	9406.798631	26.700711
210.712234	9420.798338	26.705728
211.031185	9437.143801	26.710746
211.517229	9444.934161	26.715764
211.380964	9452.917139	26.720781
211.615077	9454.261727	26.725799
211.813392	9467.053410	26.730816
211.901087	9491.930005	26.735834
212.211016	9495.762200	26.740852
212.408787	9497.244340	26.745869
213.077605	9511.370652	26.750887
213.196255	9523.517821	26.755904
213.102619	9540.360063	26.760922
213.605340	9560.575160	26.765940
213.525636	9561.256379	26.770957
213.521673	9561.186227	26.775975
213.656800	9570.403640	26.780992
213.770114	9590.955654	26.786010
213.914099	9611.023709	26.791028
214.043076	9619.500155	26.796045
214.511595	9625.915031	26.801063
214.604160	9652.996625	26.806080
214.923358	9663.230531	26.811098
215.588441	9670.098171	26.816116
215.351935	9690.400120	26.821133
215.892269	9696.749596	26.826151
216.286879	9706.415741	26.831168
216.010923	9710.004500	26.836186
216.311226	9725.558552	26.841204
216.569403	9736.119242	26.846221
216.996593	9741.453964	26.851239
217.207156	9767.314223	26.856256
217.611935	9776.587241	26.861274
217.432569	9772.902936	26.866292
217.583233	9799.302480	26.871309
218.108919	9806.300340	26.876327
218.371918	9813.072207	26.881344
218.197629	9833.949325	26.886362
218.560442	9837.510559	26.891380
218.656572	9858.556500	26.896397
218.724894	9868.721707	26.901415
218.913062	9875.824200	26.906432
219.669744	9900.097798	26.911450
219.954174	9915.121377	26.916468
219.974606	9929.663971	26.921485
220.155749	9926.175286	26.926503
220.543317	9929.440210	26.931520
220.715021	9946.640775	26.936538
221.050982	9953.051691	26.941556
221.224522	9975.454042	26.946573
221.338765	9984.068604	26.951591
221.667833	9991.344010	26.956608
221.474097	10004.155212	26.961626
221.912491	10016.485457	26.966644
222.282980	10034.616650	26.971661
222.043719	10049.339322	26.976679
222.579840	10064.021338	26.981696
222.707272	10076.764569	26.986714
223.309413	10081.322168	26.991732
223.554903	10109.686099	26.996749
223.602701	10115.661030	27.001767
224.053615	10121.166835	27.006784
223.900111	10139.126348	27.011802
224.244860	10151.393397	27.016820
224.711132	10161.894783	27.021837
225.189132	10173.790872	27.026855
225.698427	10170.689832	27.031872
224.917679	10174.838666	27.036890
225.661950	10186.979080	27.041908
226.120310	10203.886005	27.046925
226.018593	10200.385702	27.051943
226.312312	10216.681783	27.056960
226.317133	10229.810111	27.061978
226.677215	10230.349378	27.066996
227.012591	10242.455775	27.072013
226.811130	10268.878825	27.077031
227.057325	10275.264529	27.082048
227.215108	10296.960979	27.087066
227.292339	10296.986116	27.092084
227.261960	10317.298918	27.097101
227.294594	10350.084531	27.102119
228.063564	10358.352440	27.107136
227.745612	10383.544006	27.112154
228.130068	10399.377062	27.117172
228.484205	10419.471281	27.122189
228.382006	10450.232049	27.127207
228.974083	10469.270838	27.132224
228.933843	10476.257726	27.137242
229.334393	10502.043673	27.142260
229.702332	10521.189664	27.147277
229.756401	10533.475886	27.152295
230.174446	10555.273844	27.157312
230.322336	10581.264725	27.162330
230.527167	10586.773539	27.167348
230.836192	10607.199210	27.172365
230.853450	10633.102262	27.177383
231.318762	10650.037657	27.182400
231.265033	10675.386903	27.187418
231.632790	10689.705014	27.192436
231.751578	10708.053439	27.197453
231.950032	10728.656660	27.202471
232.468825	10751.437896	27.207488
232.917889	10775.273672	27.212506
233.141893	10783.356916	27.217524
233.427369	10808.009885	27.222541
233.941178	10814.555620	27.227559
234.445505	10824.290972	27.232576
234.133240	10841.806423	27.237594
234.299595	10851.325067	27.242612
234.871315	10867.064628	27.247629
234.873303	10879.855220	27.252647
235.471335	10888.947287	27.257664
235.378581	10903.956915	27.262682
235.491593	10920.040152	27.267700
236.074179	10934.493934	27.272717
236.058430	10947.010219	27.277735
236.439815	10971.838233	27.282752
236.459736	10990.675187	27.287770
236.578072	11000.290082	27.292788
236.670638	10998.647353	27.297805
236.700148	11028.665878	27.302823
237.371602	11056.994988	27.307840
237.482609	11072.606837	27.312858
237.839775	11080.476803	27.317876
238.195200	11111.268006	27.322893
237.978190	11121.945937	27.327911
238.698740	11133.227599	27.332928
238.666865	11161.553353	27.337946
239.170934	11173.779112	27.342964
239.526004	11194.891167	27.347981
239.555354	11213.335300	27.352999
239.904056	11216.788890	27.358016
240.108623	11240.602732	27.363034
240.410801	11254.023091	27.368052
241.124573	11263.134852	27.373069
240.943393	11275.733868	27.378087
240.987700	11287.646511	27.383104
241.562666	11302.176726	27.388122
241.549466	11310.031581	27.393140
242.122621	11337.370645	27.398157
242.259521	11349.528793	27.403175
242.421065	11359.321893	27.408192
242.434456	11366.013555	27.413210
242.546593	11382.314829	27.418228
242.881402	11397.405532	27.423245
243.256554	11418.446027	27.428263
243.569869	11436.880529	27.433280
243.988108	11449.335745	27.438298
244.280279	11452.696314	27.443316
244.376491	11462.942221	27.448333
244.808759	11481.294885	27.453351
245.002781	11486.599396	27.458368
245.043804	11504.447942	27.463386
245.023181	11513.329038	27.468404
245.547598	11532.442510	27.473421
245.670387	11539.954380	27.478439
246.121595	11553.569374	27.483456
246.209740	11562.945379	27.488474
246.478622	11582.592711	27.493492
246.419462	11593.167671	27.498509
246.655209	11606.643417	27.503527
247.032922	11621.102522	27.508544
247.339776	11638.797796	27.513562
247.647650	11645.523640	27.518580
248.154129	11656.215532	27.523597
248.150570	11692.105121	27.528615
248.336157	11683.045588	27.533632
248.685720	11703.908705	27.538650
248.932719	11724.138071	27.543668
249.318247	11742.256902	27.548685
249.447694	11757.411022	27.553703
249.706077	11764.706008	27.558720
249.989429	11787.833288	27.563738
250.199836	11801.221211	27.568756
250.427650	11815.226272	27.573773
250.562212	11821.196170	27.578791
250.952906	11846.344639	27.583808
251.034610	11863.726785	27.588826
251.364131	11885.898058	27.593844
251.690128	11894.404611	27.598861
252.065196	11912.411131	27.603879
252.184144	11914.089294	27.608896
252.521380	11950.129562	27.613914
252.321725	11961.794672	27.618932
252.840683	11966.377593	27.623949
252.788902	11992.600703	27.628967
253.209653	12012.944320	27.633984
253.481590	12029.579093	27.639002
253.695961	12048.307955	27.644020
254.573748	12069.968996	27.649037
254.424297	12088.137213	27.654055
254.589357	12098.690429	27.659072
254.814793	12119.183835	27.664090
255.126204	12134.946381	27.669108
255.625418	12152.210229	27.674125
255.723902	12172.600989	27.679143
256.240837	12181.861608	27.684160
256.320410	12192.734684	27.689178
256.624462	12211.028222	27.694196
257.222882	12220.132805	27.699213
257.181735	12239.985000	27.704231
257.446612	12254.708333	27.709248
257.978530	12271.462697	27.714266
257.539951	12286.242402	27.719284
258.090888	12296.700484	27.724301
258.169586	12316.727567	27.729319
258.275623	12328.391283	27.734336
258.980191	12352.045384	27.739354
258.908682	12386.594253	27.744372
259.581196	12382.154093	27.749389
259.773854	12400.573395	27.754407
260.203445	12415.855022	27.759424
260.440727	12422.086279	27.764442
260.554841	12444.195431	27.769460
261.033943	12454.261324	27.774477
261.086674	12479.933807	27.779495
261.169993	12491.044393	27.784512
261.476249	12499.622283	27.789530
261.818749	12516.537402	27.794548
262.182046	12522.864480	27.799565
262.257675	12538.918485	27.804583
262.543141	12551.208989	27.809600
262.863648	12557.846469	27.814618
262.791500	12571.320319	27.819636
263.116004	12589.790536	27.824653
263.395438	12614.736417	27.829671
263.492341	12619.162358	27.834688
264.055889	12649.516386	27.839706
264.022750	12658.990277	27.844724
264.665101	12675.844996	27.849741
264.664718	12687.916537	27.854759
264.639210	12709.627622	27.859776
265.375124	12719.210846	27.864794
265.000898	12749.701085	27.869812
265.642565	12776.541241	27.874829
265.579933	12785.021082	27.879847
265.722056	12811.976916	27.884864
266.171438	12833.075545	27.889882
266.082283	12867.524361	27.894900
266.578661	12881.787730	27.899917
267.024005	12914.118821	27.904935
267.498176	12942.866756	27.909952
267.662606	12949.443519	27.914970
268.127745	12977.504418	27.919988
268.526634	12996.692373	27.925005
269.111826	13019.834584	27.930023
269.425040	13021.089202	27.935040
270.250789	13026.206342	27.940058
270.049599	13040.805699	27.945076
270.395054	13045.923408	27.950093
270.665069	13076.534732	27.955111
271.011579	13077.019623	27.960128
271.510995	13069.772347	27.965146
271.728353	13094.234445	27.970164
271.771313	13097.021211	27.975181
272.119505	13093.843819	27.980199
272.153299	13120.422556	27.985216
272.589740	13128.251284	27.990234
272.486088	13139.137936	27.995252
272.882215	13163.324790	28.000269
272.778612	13167.270315	28.005287
273.002399	13194.772684	28.010304
273.346194	13202.894086	28.015322
273.517280	13226.549369	28.020340
273.735588	13250.855549	28.025357
274.047483	13279.199138	28.030375
273.990397	13300.194537	28.035392
274.468181	13323.818202	28.040410
274.838295	13357.877035	28.045428
275.198785	13361.473328	28.050445
275.746008	13392.663455	28.055463
275.894873	13408.302042	28.060480
276.333143	13435.257262	28.065498
276.565121	13445.567092	28.070516
276.690756	13467.329859	28.075533
277.220239	13474.612351	28.080551
277.547594	13489.923708	28.085568
277.991074	13508.513990	28.090586
277.489015	13534.417683	28.095604
277.930190	13536.374485	28.100621
278.175046	13577.011283	28.105639
278.527108	13609.362330	28.110656
278.753085	13615.670767	28.115674
279.002453	13642.126501	28.120692
279.309031	13657.934671	28.125709
279.456541	13678.665119	28.130727
279.640811	13710.470500	28.135744
280.417335	13712.296283	28.140762
280.625520	13736.940509	28.145780
280.921086	13754.104202	28.150797
281.275353	13770.664139	28.155815
281.198209	13779.876493	28.160832
281.903575	13791.928386	28.165850
281.852298	13820.413288	28.170868
282.340411	13839.284950	28.175885
282.494919	13847.340248	28.180903
282.268485	13876.205590	28.185920
282.752380	13889.011139	28.190938
282.711681	13929.423381	28.195956
283.188902	13943.556912	28.200973
283.961036	13973.466107	28.205991
284.345892	13998.160334	28.211008
284.436212	14014.177920	28.216026
284.345097	14033.854622	28.221044
284.796277	14056.620201	28.226061
285.232054	14072.535074	28.231079
285.414736	14106.596506	28.236096
285.664635	14126.672398	28.241114
285.932879	14155.376143	28.246132
286.011466	14170.960891	28.251149
286.388424	14198.683915	28.256167
286.381835	14222.078473	28.261184
287.258647	14237.977377	28.266202
287.351223	14267.991505	28.271220
287.911178	14297.206734	28.276237
288.320228	14305.546410	28.281255
288.817417	14324.754371	28.286272
288.846440	14345.629738	28.291290
289.023481	14367.637357	28.296308
289.372666	14388.409458	28.301325
289.794807	14411.106267	28.306343
290.029657	14437.379745	28.311360
290.431894	14452.856139	28.316378
290.628821	14477.804341	28.321396
291.044404	14494.945839	28.326413
291.228060	14522.750203	28.331431
291.264666	14548.111087	28.336448
291.555159	14549.349096	28.341466
291.988135	14582.634242	28.346484
291.889965	14605.486620	28.351501
292.427871	14633.788936	28.356519
292.650733	14651.235066	28.361536
292.740077	14682.317366	28.366554
293.338332	14708.006473	28.371572
293.136498	14725.778140	28.376589
294.056274	14759.545819	28.381607
294.228406	14789.480002	28.386624
294.668972	14807.761806	28.391642
294.674272	14835.986994	28.396660
295.089745	14866.412196	28.401677
295.254157	14879.129478	28.406695
295.306874	14912.512789	28.411712
295.963070	14934.137865	28.416730
296.315414	14956.218178	28.421748
296.583514	14986.125836	28.426765
297.176001	15000.606861	28.431783
297.278873	15022.859279	28.436800
297.570726	15040.582823	28.441818
297.746195	15078.087720	28.446836
298.169205	15108.288347	28.451853
298.645610	15115.580353	28.456871
298.659227	15152.133506	28.461888
299.217875	15165.337459	28.466906
299.420558	15177.427733	28.471924
299.713271	15202.321821	28.476941
299.947379	15224.631631	28.481959
300.317693	15247.454790	28.486976
300.676251	15260.773826	28.491994
300.976462	15281.980664	28.497012
301.319500	15288.301935	28.502029
301.558501	15308.633238	28.507047
301.699452	15328.471733	28.512064
302.248468	15331.362819	28.517082
302.487516	15357.695398	28.522100
302.792142	15388.354218	28.527117
303.440205	15391.673371	28.532135
303.579089	15408.574722	28.537152
303.703796	15418.518994	28.542170
303.677560	15445.801718	28.547188
303.871443	15466.121760	28.552205
304.320910	15481.821424	28.557223
304.578523	15520.450038	28.562240
305.004668	15548.484006	28.567258
305.038242	15561.191916	28.572276
304.633551	15598.730815	28.577293
305.709921	15616.765078	28.582311
306.191658	15653.076539	28.587328
306.444434	15668.364449	28.592346
307.063506	15702.691233	28.597364
307.587225	15716.938405	28.602381
308.004030	15722.549496	28.607399
308.099498	15750.439866	28.612416
308.353728	15762.570914	28.617434
308.778913	15793.511592	28.622452
308.784522	15813.763883	28.627469
309.580434	15831.797439	28.632487
309.878131	15855.399381	28.637504
310.081738	15860.837709	28.642522
310.633246	15885.078597	28.647540
310.778947	15900.928136	28.652557
310.742274	15911.591236	28.657575
311.215001	15939.049242	28.662592
311.146233	15954.563902	28.667610
311.526900	15992.096886	28.672628
311.773108	16021.983267	28.677645
312.122339	16037.808771	28.682663
312.281619	16077.819779	28.687680
312.627137	16087.450600	28.692698
313.050987	16115.000506	28.697716
312.656749	16166.229923	28.702733
313.545199	16186.598447	28.707751
313.653953	16212.098142	28.712768
314.376327	16243.808539	28.717786
314.817111	16270.791687	28.722804
314.884206	16295.504069	28.727821
314.988147	16308.806135	28.732839
315.356953	16349.465620	28.737856
315.733154	16385.153114	28.742874
316.264266	16398.786577	28.747892
316.236023	16422.397477	28.752909
317.030342	16453.604667	28.757927
317.314119	16482.182280	28.762944
317.265194	16506.614695	28.767962
317.563263	16537.823647	28.772980
317.816265	16554.395267	28.777997
318.571606	16583.796665	28.783015
318.936256	16613.191736	28.788032
319.270073	16633.062994	28.793050
319.397046	16652.853393	28.798068
320.092075	16690.884521	28.803085
320.283325	16704.999928	28.808103
320.447444	16732.261226	28.813120
320.955815	16759.762003	28.818138
321.372084	16774.067253	28.823156
321.223420	16787.761330	28.828173
321.551752	16813.394326	28.833191
321.915545	16836.747198	28.838208
322.021140	16856.018110	28.843226
322.658811	16883.987901	28.848244
322.639260	16920.312487	28.853261
322.831628	16934.974815	28.858279
323.385695	16959.719651	28.863296
323.148219	16994.371901	28.868314
323.582533	17017.774849	28.873332
323.813428	17058.108975	28.878349
324.371871	17084.538146	28.883367
324.732027	17114.369865	28.888384
324.768021	17153.937330	28.893402
325.494370	17172.671054	28.898420
325.558992	17214.880254	28.903437
326.076776	17239.169700	28.908455
326.348446	17268.381135	28.913472
326.818310	17305.680154	28.918490
327.308647	17344.238367	28.923508
327.597045	17368.080445	28.928525
328.097180	17387.483820	28.933543
328.600839	17417.687997	28.938560
328.683954	17455.048093	28.943578
329.375884	17469.234332	28.948596
329.530389	17499.094418	28.953613
329.649746	17527.562310	28.958631
330.272250	17547.079632	28.963648
330.188153	17576.061947	28.968666
330.932820	17606.385849	28.973684
331.076439	17631.011939	28.978701
331.616717	17646.333009	28.983719
331.999244	17675.211618	28.988736
332.252914	17699.914202	28.993754
333.054513	17718.773246	28.998772
333.187308	17735.353308	29.003789
333.653248	17765.846491	29.008807
333.794986	17781.501478	29.013824
333.929505	17805.536686	29.018842
334.301429	17824.283997	29.023860
334.665355	17849.238118	29.028877
334.800103	17868.614157	29.033895
335.466204	17891.294413	29.038912
335.460545	17922.551440	29.043930
336.201304	17940.296961	29.048948
336.453492	17974.446377	29.053965
336.355951	18003.501017	29.058983
336.643199	18025.276253	29.064000
336.823484	18062.107827	29.069018
337.497170	18094.241237	29.074036
337.616779	18126.811435	29.079053
337.857684	18150.894197	29.084071
338.328226	18183.863637	29.089088
338.750160	18210.266730	29.094106
339.219000	18234.631933	29.099124
339.485934	18269.457302	29.104141
340.150625	18285.674207	29.109159
340.501655	18315.487543	29.114176
340.878320	18332.986269	29.119194
341.308596	18349.156845	29.124212
341.558508	18381.972405	29.129229
341.838338	18396.783939	29.134247
342.314334	18425.024228	29.139264
342.317330	18453.235518	29.144282
342.780654	18472.072499	29.149300
343.257623	18500.918037	29.154317
343.140026	18528.876686	29.159335
343.857419	18546.283098	29.164352
344.229186	18558.912235	29.169370
344.808178	18570.772610	29.174388
345.150314	18598.095856	29.179405
345.228622	18617.988078	29.184423
345.684136	18617.988575	29.189440
346.055273	18658.743225	29.194458
346.267140	18676.665185	29.199476
346.254292	18700.278378	29.204493
346.256687	18723.647917	29.209511
346.939242	18753.910109	29.214528
346.775155	18781.192758	29.219546
347.370723	18817.490832	29.224564
347.448395	18856.086072	29.229581
347.884828	18898.750446	29.234599
348.577223	18920.825633	29.239616
348.243786	18964.670321	29.244634
348.904169	18996.418340	29.249652
349.144167	19025.896630	29.254669
349.776754	19056.777661	29.259687
350.168475	19091.130167	29.264704
350.149136	19134.166785	29.269722
350.851971	19175.436960	29.274740
351.595497	19206.356691	29.279757
351.388875	19232.877863	29.284775
351.959043	19261.343624	29.289792
352.156869	19301.510565	29.294810
352.510389	19329.030177	29.299828
353.031354	19373.401587	29.304845
353.144406	19413.689994	29.309863
353.787668	19434.493996	29.314880
353.989038	19466.099631	29.319898
354.557261	19502.799386	29.324916
355.128190	19539.878677	29.329933
355.168923	19571.482675	29.334951
356.190652	19593.387706	29.339968
356.101200	19636.222821	29.344986
356.725165	19661.191892	29.350004
356.994929	19698.007590	29.355021
356.736801	19734.637864	29.360039
357.591828	19755.672117	29.365056
357.505411	19799.341050	29.370074
358.312285	19828.296769	29.375092
358.574980	19864.321084	29.380109
358.600893	19891.853186	29.385127
359.167901	19925.945158	29.390144
359.403988	19954.982777	29.395162
359.901641	19991.080476	29.400180
360.399729	20019.970886	29.405197
360.863786	20052.639296	29.410215
361.392898	20092.222172	29.415232
361.401884	20119.672321	29.420250
362.056612	20149.203900	29.425268
362.430196	20190.786369	29.430285
362.560312	20210.665632	29.435303
363.259026	20234.929595	29.440320
363.657448	20264.294055	29.445338
363.705706	20296.010110	29.450356
364.309296	20325.045993	29.455373
364.607807	20357.482239	29.460391
365.058141	20390.025888	29.465408
365.227832	20431.614264	29.470426
365.635747	20449.959765	29.475444
366.328101	20471.095893	29.480461
366.412422	20497.716045	29.485479
367.219748	20525.734922	29.490496
367.530307	20555.746565	29.495514
367.842265	20569.257316	29.500532
367.639036	20601.956637	29.505549
368.097097	20633.514201	29.510567
368.548768	20644.708190	29.515584
368.639870	20689.664893	29.520602
368.983457	20718.066534	29.525620
369.675046	20744.058647	29.530637
369.435994	20766.622798	29.535655
370.084110	20798.551278	29.540672
370.446742	20824.153293	29.545690
370.740615	20864.434252	29.550708
370.939436	20903.291683	29.555725
371.658315	20933.018998	29.560743
372.306423	20955.542475	29.565760
372.818450	20993.099798	29.570778
372.865893	21014.548095	29.575796
373.295877	21051.430175	29.580813
373.280639	21082.021556	29.585831
373.764971	21101.129212	29.590848
374.218447	21143.496990	29.595866
374.404388	21182.697722	29.600884
374.754000	21207.744391	29.605901
375.179949	21255.701002	29.610919
375.418907	21287.138344	29.615936
376.238797	21327.995664	29.620954
376.296087	21358.660701	29.625972
376.925308	21385.695164	29.630989
377.398196	21418.005342	29.636007
377.711031	21460.743993	29.641024
378.105419	21492.280590	29.646042
378.746736	21519.220256	29.651060
379.306131	21544.018365	29.656077
379.520684	21585.110316	29.661095
379.895190	21610.974857	29.666112
380.172133	21646.406303	29.671130
380.507950	21679.906278	29.676148
381.082053	21709.761369	29.681165
380.953881	21744.436980	29.686183
381.401767	21768.932224	29.691200
382.304412	21798.894011	29.696218
382.639715	21847.245665	29.701236
383.008051	21879.113645	29.706253
382.885251	21907.565970	29.711271
383.528055	21948.105634	29.716288
383.603643	21983.337719	29.721306
383.949298	22020.005681	29.726324
384.492137	22052.972424	29.731341
384.736834	22101.311397	29.736359
385.181131	22127.745394	29.741376
385.433975	22183.561058	29.746394
385.658100	22222.311733	29.751412
386.236703	22252.409844	29.756429
386.584247	22293.096865	29.761447
386.949799	22329.677078	29.766464
387.255548	22366.878978	29.771482
387.399396	22407.543166	29.776500
388.138254	22459.859767	29.781517
388.477100	22505.100464	29.786535
389.039378	22535.813513	29.791552
389.295509	22582.343578	29.796570
389.540927	22624.806224	29.801588
390.214274	22653.156672	29.806605
391.003227	22712.872870	29.811623
391.516352	22738.788776	29.816640
391.762022	22769.846234	29.821658
392.147476	22799.147910	29.826676
393.236146	22829.637372	29.831693
393.457797	22856.648512	29.836711
394.143014	22883.504286	29.841728
394.459769	22897.976317	29.846746
394.468965	22908.492846	29.851764
394.908273	22928.619094	29.856781
394.804872	22960.917072	29.861799
395.371073	22972.290788	29.866816
395.849313	23010.961883	29.871834
396.082063	23035.869763	29.876852
396.433550	23077.489848	29.881869
396.443039	23115.694659	29.886887
396.604078	23141.995721	29.891904
397.136915	23179.155596	29.896922
397.447870	23232.477110	29.901940
398.006586	23270.072809	29.906957
398.069791	23314.490870	29.911975
398.287353	23364.972811	29.916992
398.484578	23410.461647	29.922010
398.776388	23448.198012	29.927028
399.307890	23494.103293	29.932045
399.764252	23546.119899	29.937063
399.962867	23588.707802	29.942080
400.636408	23636.173046	29.947098
401.285652	23696.319449	29.952116
402.006179	23722.957869	29.957133
402.573076	23760.811895	29.962151
403.409941	23797.263827	29.967168
403.774947	23828.658289	29.972186
404.264745	23865.041558	29.977204
405.310134	23879.223779	29.982221
405.275107	23922.535431	29.987239
405.731612	23946.385949	29.992256
405.855999	23975.163579	29.997274
406.255005	24008.604135	30.002292
406.796965	24034.227144	30.007309
407.027094	24061.372835	30.012327
407.937647	24112.023198	30.017344
407.770984	24132.254135	30.022362
407.957363	24174.053986	30.027380
408.732726	24198.224309	30.032397
409.123352	24240.854666	30.037415
409.079607	24279.950747	30.042432
409.896986	24314.005550	30.047450
409.985783	24359.623645	30.052468
410.453255	24388.778924	30.057485
410.493401	24438.730451	30.062503
410.869914	24480.211091	30.067520
411.625138	24520.047724	30.072538
411.401377	24576.268535	30.077556
412.330533	24608.044298	30.082573
412.633033	24654.082008	30.087591
413.066506	24696.555056	30.092608
413.531238	24738.989933	30.097626
413.619984	24791.242961	30.102644
414.229290	24839.403385	30.107661
414.561910	24877.700703	30.112679
414.802104	24925.903421	30.117696
415.291296	24969.334560	30.122714
415.737924	25028.497351	30.127732
416.100557	25055.537593	30.132749
416.624627	25113.275011	30.137767
417.224002	25159.712881	30.142784
418.081149	25200.084605	30.147802
418.225864	25252.433876	30.152820
418.503345	25283.479648	30.157837
419.063442	25319.737734	30.162855
419.081133	25359.590937	30.167872
419.819064	25408.744094	30.172890
420.677433	25452.880282	30.177908
420.968463	25483.708145	30.182925
421.457618	25518.751538	30.187943
421.772858	25550.151095	30.192960
422.597445	25583.615913	30.197978
422.668312	25622.680373	30.202996
423.170804	25651.433072	30.208013
423.317521	25670.701028	30.213031
423.247241	25719.141776	30.218048
423.841390	25757.549256	30.223066
424.053617	25800.347028	30.228084
424.827436	25837.526537	30.233101
425.249109	25888.177796	30.238119
425.475199	25931.878775	30.243136
426.105809	25963.818356	30.248154
426.240024	26011.625332	30.253172
426.401055	26055.416222	30.258189
426.860799	26101.151165	30.263207
427.507298	26153.951749	30.268224
427.953587	26202.972441	30.273242
427.988836	26262.753097	30.278260
428.524126	26295.718311	30.283277
428.891726	26353.968329	30.288295
429.265951	26405.701311	30.293312
429.942137	26455.905345	30.298330
430.347408	26515.442829	30.303348
430.898221	26564.071961	30.308365
431.343146	26607.019399	30.313383
431.756223	26653.296557	30.318400
432.815433	26696.691552	30.323418
433.323200	26744.681729	30.328436
433.743866	26770.194849	30.333453
433.943855	26817.646263	30.338471
434.703455	26863.652272	30.343488
435.094781	26900.367391	30.348506
435.690474	26943.060519	30.353524
436.140462	26976.917973	30.358541
436.970998	27017.951292	30.363559
437.019718	27048.213258	30.368576
437.479471	27086.469294	30.373594
437.891089	27125.547128	30.378612
438.225009	27158.276012	30.383629
438.552458	27198.090209	30.388647
439.118018	27249.043446	30.393664
439.535165	27281.670501	30.398682
439.178867	27320.402503	30.403700
439.826968	27367.655248	30.408717
440.443295	27408.371619	30.413735
440.762882	27466.182296	30.418752
441.373509	27511.224236	30.423770
441.693868	27557.474987	30.428788
442.364204	27607.191302	30.433805
442.775479	27643.292798	30.438823
443.419992	27692.486872	30.443840
444.110858	27738.610669	30.448858
444.339875	27775.521643	30.453876
444.628243	27814.290207	30.458893
445.412317	27854.951538	30.463911
445.397037	27897.602864	30.468928
445.901663	27936.664023	30.473946
446.056330	27985.652809	30.478964
446.457939	28028.897995	30.483981
447.250816	28091.575357	30.488999
447.352824	28133.687433	30.494016
447.780621	28173.077250	30.499034
448.266615	28226.308163	30.504052
448.399806	28281.297700	30.509069
449.156210	28334.651460	30.514087
449.437969	28384.885276	30.519104
449.949419	28435.854115	30.524122
450.263872	28491.240218	30.529140
450.570377	28534.366742	30.534157
451.184033	28574.237782	30.539175
451.126064	28628.480866	30.544192
452.092117	28679.857955	30.549210
452.975485	28720.763589	30.554228
453.235562	28782.752328	30.559245
453.625484	28816.869366	30.564263
454.034507	28852.910675	30.569280
455.072354	28907.311150	30.574298
455.165146	28948.685437	30.579316
455.874587	28996.008221	30.584333
456.350499	29036.250070	30.589351
456.768616	29078.990442	30.594368
457.124432	29126.258432	30.599386
457.620193	29164.257616	30.604404
458.115150	29202.197081	30.609421
458.768430	29247.160799	30.614439
458.682555	29292.032221	30.619456
459.301072	29336.099721	30.624474
459.597186	29382.523395	30.629492
459.953983	29446.384940	30.634509
460.682897	29492.062346	30.639527
460.896432	29543.194063	30.644544
461.629557	29594.650200	30.649562
461.906474	29642.342722	30.654580
462.535152	29694.541960	30.659597
463.159645	29747.808301	30.664615
463.697994	29796.950190	30.669632
463.808902	29845.746412	30.674650
464.061670	29888.456151	30.679668
464.341509	29950.758104	30.684685
465.331252	29993.870039	30.689703
465.743659	30062.251573	30.694720
466.017885	30104.276892	30.699738
467.066531	30154.909679	30.704756
467.416782	30207.768455	30.709773
467.902984	30254.702509	30.714791
467.898689	30305.500193	30.719808
468.504085	30334.000805	30.724826
469.624316	30389.102131	30.729844
470.043457	30455.774242	30.734861
470.770665	30482.516724	30.739879
471.062350	30526.729561	30.744896
471.419232	30561.558991	30.749914
472.178174	30610.436443	30.754932
472.881388	30645.240382	30.759949
473.778726	30670.592195	30.764967
473.931448	30720.178958	30.769984
474.478824	30747.863282	30.775002
474.988345	30784.926768	30.780020
475.380349	30811.974352	30.785037
475.671839	30843.064100	30.790055
476.004797	30898.003681	30.795072
476.572573	30929.814565	30.800090
476.553978	30961.018838	30.805108
476.805849	31011.038034	30.810125
477.704759	31050.832943	30.815143
477.963023	31106.201953	30.820160
478.566154	31150.188254	30.825178
479.167533	31195.550474	30.830196
479.365173	31237.543850	30.835213
479.480096	31293.552328	30.840231
479.916915	31353.792153	30.845248
480.784327	31405.673144	30.850266
481.224920	31457.482818	30.855284
481.434389	31505.387178	30.860301
481.893858	31548.111004	30.865319
482.279759	31599.466358	30.870336
482.464132	31647.331081	30.875354
483.166264	31686.084106	30.880372
483.564223	31732.768537	30.885389
484.429899	31785.231453	30.890407
484.290032	31834.645697	30.895424
484.899972	31878.108977	30.900442
485.232249	31941.948995	30.905460
485.816211	31993.910098	30.910477
486.110492	32043.991491	30.915495
486.348467	32110.772395	30.920512
486.932747	32178.729971	30.925530
487.762321	32226.423445	30.930548
488.048895	32295.225716	30.935565
489.013026	32333.703423	30.940583
489.423657	32396.399482	30.945600
489.583809	32454.107930	30.950618
490.358528	32502.085706	30.955636
490.482060	32571.616418	30.960653
491.211570	32633.399306	30.965671
491.667583	32691.640205	30.970688
492.027534	32747.003901	30.975706
492.452262	32817.782596	30.980724
493.262674	32881.758443	30.985741
493.692523	32943.023984	30.990759
494.295854	33007.592958	30.995776
494.246926	33063.164010	31.000794
494.720103	33125.644089	31.005812
495.493148	33186.434145	31.010829
495.956453	33257.959175	31.015847
496.425995	33318.916562	31.020864
497.010735	33387.837918	31.025882
497.578138	33446.400520	31.030900
498.116517	33519.353007	31.035917
498.449275	33576.433955	31.040935
499.152014	33642.686374	31.045952
499.467552	33702.029764	31.050970
500.293454	33760.026928	31.055988
500.131740	33833.569643	31.061005
500.836375	33896.162514	31.066023
501.517350	33971.415643	31.071040
502.006464	34043.854639	31.076058
502.667494	34109.345783	31.081076
502.660729	34172.211746	31.086093
503.636342	34234.697947	31.091111
503.924276	34300.529098	31.096128
504.198288	34371.780661	31.101146
504.890858	34437.646459	31.106164
505.264244	34524.848749	31.111181
506.019788	34588.723081	31.116199
506.912669	34652.783220	31.121216
507.629466	34715.231821	31.126234
508.421780	34768.040743	31.131252
508.725251	34830.501220	31.136269
509.410041	34889.150175	31.141287
510.199501	34932.218972	31.146304
510.467937	34993.221643	31.151322
511.078765	35046.692476	31.156340
511.405633	35103.145040	31.161357
511.913668	35141.205625	31.166375
512.703661	35206.042089	31.171392
512.794559	35260.107488	31.176410
513.643890	35301.270784	31.181428
513.952026	35366.597647	31.186445
514.557840	35421.446278	31.191463
515.114989	35477.249802	31.196480
515.716308	35535.078432	31.201498
516.243000	35579.605922	31.206516
516.522777	35631.599550	31.211533
517.252965	35679.905705	31.216551
517.751514	35726.770242	31.221568
517.796069	35769.632757	31.226586
518.855430	35819.910865	31.231604
519.114726	35872.549180	31.236621
519.592890	35921.033309	31.241639
520.204077	35964.257121	31.246656
520.658231	36027.208124	31.251674
520.799835	36076.764406	31.256692
521.411593	36126.808048	31.261709
521.787183	36189.782066	31.266727
522.441481	36243.845745	31.271744
522.465260	36296.274901	31.276762
523.156896	36354.561476	31.281780
523.555618	36431.446351	31.286797
524.576639	36498.278522	31.291815
524.609438	36561.998432	31.296832
525.048951	36626.677033	31.301850
525.560683	36688.961283	31.306868
525.799474	36762.768651	31.311885
526.972090	36832.704478	31.316903
527.408309	36896.945933	31.321920
527.829758	36957.330411	31.326938
528.744473	37016.816244	31.331956
529.189320	37091.670245	31.336973
529.496440	37146.908024	31.341991
530.033124	37216.524334	31.347008
530.565066	37300.365529	31.352026
531.306759	37351.978569	31.357044
532.222485	37400.523822	31.362061
532.908608	37462.750391	31.367079
533.863401	37517.550957	31.372096
534.078665	37577.431899	31.377114
535.055934	37616.108254	31.382132
535.312076	37677.409288	31.387149
535.626522	37724.287362	31.392167
536.534016	37782.303061	31.397184
536.779087	37834.785363	31.402202
537.261177	37885.884194	31.407220
537.743947	37955.474393	31.412237
538.235009	38013.303977	31.417255
538.928408	38061.187087	31.422272
539.173456	38128.270262	31.427290
539.580868	38189.494397	31.432308
539.912438	38247.398414	31.437325
540.667069	38311.153622	31.442343
541.022330	38381.482961	31.447360
541.532399	38447.488336	31.452378
542.272126	38507.118461	31.457396
542.578906	38588.032886	31.462413
543.106318	38660.888218	31.467431
543.703288	38716.673134	31.472448
544.080899	38785.469598	31.477466
544.696150	38864.601555	31.482484
545.383911	38928.590918	31.487501
545.712427	38984.263187	31.492519
546.356425	39062.087731	31.497536
546.465580	39143.090930	31.502554
547.283093	39202.338057	31.507572
547.850165	39273.847884	31.512589
548.162834	39350.339621	31.517607
548.804592	39431.413952	31.522624
549.325510	39506.303261	31.527642
550.186518	39566.393446	31.532660
550.453059	39646.381801	31.537677
551.245169	39707.989413	31.542695
551.679462	39769.817308	31.547712
552.226553	39848.747019	31.552730
552.965604	39905.477977	31.557748
553.758486	39966.417182	31.562765
554.446820	40033.440495	31.567783
554.866554	40082.939731	31.572800
555.121955	40147.020579	31.577818
555.323152	40206.663165	31.582836
556.181890	40275.363706	31.587853
556.755367	40333.540596	31.592871
556.990659	40401.852174	31.597888
557.987698	40480.233675	31.602906
558.228435	40541.578490	31.607924
558.936315	40615.500839	31.612941
559.536934	40694.652639	31.617959
559.877300	40764.261335	31.622976
560.391388	40831.635170	31.627994
560.966203	40905.410214	31.633012
561.536504	40973.545490	31.638029
562.233975	41048.541391	31.643047
562.769930	41119.760563	31.648064
563.277041	41197.721003	31.653082
563.960610	41264.989525	31.658100
564.353276	41354.260806	31.663117
564.791001	41429.029692	31.668135
565.721732	41496.261398	31.673152
566.089362	41569.868153	31.678170
566.678829	41640.679612	31.683188
567.270204	41713.561829	31.688205
567.847622	41789.833803	31.693223
569.063657	41859.592448	31.698240
569.275894	41937.904622	31.703258
569.834699	42010.866004	31.708276
570.348793	42079.563946	31.713293
570.710241	42160.955532	31.718311
571.326408	42229.103678	31.723328
572.142105	42303.144452	31.728346
572.784859	42377.425594	31.733364
573.257752	42446.794645	31.738381
573.892178	42530.661932	31.743399
574.588861	42596.856678	31.748416
575.045197	42666.516564	31.753434
575.886845	42741.113579	31.758452
576.446280	42806.116344	31.763469
576.979342	42887.236553	31.768487
577.481745	42955.283053	31.773504
577.874971	43023.439385	31.778522
578.396901	43100.789836	31.783540
579.247818	43178.335674	31.788557
579.798222	43251.918959	31.793575
580.545230	43313.599809	31.798592
580.980521	43398.529944	31.803610
581.377495	43459.262009	31.808628
581.951427	43546.499796	31.813645
582.558158	43620.214150	31.818663
583.259340	43688.934536	31.823680
584.160776	43762.152482	31.828698
585.054104	43822.058692	31.833716
585.899523	43884.463945	31.838733
585.963072	43950.607094	31.843751
586.605073	44014.915379	31.848768
587.222319	44092.730951	31.853786
587.588183	44164.296211	31.858804
588.515648	44225.640895	31.863821
588.816366	44294.931650	31.868839
589.371167	44357.585392	31.873856
589.973522	44430.773286	31.878874
590.384036	44494.872047	31.883892
590.601603	44560.521507	31.888909
591.149379	44648.232896	31.893927
591.848389	44711.981665	31.898944
592.372402	44785.771136	31.903962
592.687593	44853.631353	31.908980
593.318297	44939.420283	31.913997
593.556617	45013.804046	31.919015
594.277011	45095.423913	31.924032
594.792982	45173.409119	31.929050
595.120795	45253.683203	31.934068
595.716833	45334.876317	31.939085
596.431457	45423.334179	31.944103
597.221833	45501.853229	31.949120
597.729352	45596.821850	31.954138
598.466153	45672.499360	31.959156
599.145659	45743.763130	31.964173
599.815957	45838.747140	31.969191
600.657566	45905.608584	31.974208
601.296310	45997.033880	31.979226
601.186384	46078.271034	31.984244
602.457861	46155.652466	31.989261
603.229080	46234.755570	31.994279
604.253468	46306.725474	31.999296
604.499380	46393.484505	32.004314
605.051186	46467.326537	32.009332
605.931893	46534.853162	32.014349
606.596353	46615.200621	32.019367
607.028240	46688.122378	32.024384
607.722108	46766.975264	32.029402
608.156857	46855.413481	32.034420
608.811526	46923.559830	32.039437
609.432992	47007.124176	32.044455
610.121774	47079.774518	32.049472
610.665698	47163.990206	32.054490
611.421399	47249.541712	32.059508
612.081191	47316.349794	32.064525
612.380599	47400.666916	32.069543
612.809584	47479.452854	32.074560
613.674207	47557.330383	32.079578
613.994463	47648.320542	32.084596
614.636579	47736.166567	32.089613
615.153703	47827.399796	32.094631
615.863254	47909.598919	32.099648
616.673887	47985.270383	32.104666
616.798909	48077.554799	32.109684
617.420334	48159.791667	32.114701
618.071176	48250.925908	32.119719
619.095989	48347.212400	32.124736
619.454967	48429.174840	32.129754
620.264942	48512.436818	32.134772
621.399545	48593.185567	32.139789
622.056484	48674.468283	32.144807
622.358294	48762.542637	32.149824
623.419776	48836.448701	32.154842
623.928304	48918.183289	32.159860
625.041646	48981.723366	32.164877
625.759354	49060.117660	32.169895
626.243861	49125.754738	32.174912
626.676163	49202.778831	32.179930
627.046360	49280.097712	32.184948
627.670448	49351.801111	32.189965
628.320736	49436.157754	32.194983
628.842318	49514.788423	32.200000
629.486142	49594.539279	32.205018
629.708082	49679.109851	32.210036
630.534050	49763.195756	32.215053
631.273552	49850.710195	32.220071
631.790215	49921.441841	32.225088
632.446255	50005.594775	32.230106
632.657160	50079.358752	32.235124
633.386218	50160.462201	32.240141
633.258653	50255.761208	32.245159
634.394562	50343.803010	32.250176
634.863390	50414.828614	32.255194
635.728286	50517.456202	32.260212
636.161562	50601.853829	32.265229
636.427980	50683.566477	32.270247
636.895826	50777.702267	32.275264
638.023205	50869.904129	32.280282
638.275456	50965.563980	32.285300
639.194695	51068.330819	32.290317
639.561629	51158.808906	32.295335
640.480081	51253.494793	32.300352
640.993454	51351.832745	32.305370
641.334557	51444.953645	32.310388
642.592798	51536.006408	32.315405
643.161876	51643.448507	32.320423
643.851210	51733.427561	32.325440
644.511506	51830.265565	32.330458
645.288063	51929.943224	32.335476
646.050982	52013.468256	32.340493
646.526983	52104.741329	32.345511
647.163592	52199.383658	32.350528
647.754919	52290.114256	32.355546
648.763811	52388.094552	32.360564
649.444175	52486.900276	32.365581
649.898839	52579.300385	32.370599
650.322954	52670.758417	32.375616
651.337905	52764.867249	32.380634
651.618040	52862.667078	32.385652
652.418262	52948.479952	32.390669
653.497579	53056.199398	32.395687
653.672393	53151.396435	32.400704
654.951060	53223.821097	32.405722
655.950085	53319.211337	32.410740
656.839002	53400.519969	32.415757
657.422011	53479.415696	32.420775
658.529705	53548.995417	32.425792
659.238788	53632.855350	32.430810
659.547403	53723.073935	32.435828
660.626458	53782.911440	32.440845
660.989029	53862.312616	32.445863
661.880485	53947.021913	32.450880
662.504195	54017.277083	32.455898
662.913796	54103.563889	32.460916
663.319953	54181.139711	32.465933
663.962933	54258.392439	32.470951
664.434403	54336.766746	32.475968
665.317214	54423.077898	32.480986
665.816141	54512.535856	32.486004
666.548861	54603.705618	32.491021
667.139765	54689.750269	32.496039
667.919469	54793.485457	32.501056
668.867731	54874.329241	32.506074
669.373703	54948.006177	32.511092
669.760307	55029.777310	32.516109
670.534122	55117.796394	32.521127
671.118929	55208.620646	32.526144
671.875519	55290.723475	32.531162
672.164607	55395.680101	32.536180
673.266441	55463.890304	32.541197
673.621435	55565.709552	32.546215
674.358611	55665.558160	32.551232
675.055681	55738.909559	32.556250
675.426608	55836.930416	32.561268
675.920041	55930.281382	32.566285
676.594152	56014.732251	32.571303
677.128437	56109.764270	32.576320
677.816697	56199.047011	32.581338
678.180848	56298.379154	32.586356
678.992008	56390.409860	32.591373
679.640200	56481.646528	32.596391
680.353773	56579.191163	32.601408
681.375114	56672.730151	32.606426
681.891791	56777.012074	32.611444
682.447835	56867.128427	32.616461
682.894721	56974.354669	32.621479
683.437409	57070.622026	32.626496
684.301116	57165.389893	32.631514
684.641255	57267.340422	32.636532
685.284886	57371.130615	32.641549
686.084927	57481.669092	32.646567
686.859816	57603.099404	32.651584
687.627434	57705.607138	32.656602
688.281641	57813.890497	32.661620
689.044407	57913.032216	32.666637
690.028024	58013.212154	32.671655
690.450551	58113.984443	32.676672
691.424297	58218.564953	32.681690
691.705116	58342.362480	32.686708
692.590971	58433.271890	32.691725
693.416980	58545.202157	32.696743
694.024729	58657.295475	32.701760
695.063976	58747.384792	32.706778
695.585318	58865.174357	32.711796
696.228043	58968.328483	32.716813
697.056282	59081.234528	32.721831
697.542050	59186.153460	32.726848
698.149407	59288.297690	32.731866
698.670118	59401.774502	32.736884
699.365397	59521.574001	32.741901
700.197812	59628.820372	32.746919
700.560392	59752.404585	32.751936
701.041538	59874.434366	32.756954
701.798435	59993.139568	32.761972
702.806369	60109.453176	32.766989
703.550618	60243.170670	32.772007
704.008680	60346.381335	32.777024
704.611723	60465.032576	32.782042
705.765649	60596.890006	32.787060
706.433102	60713.737304	32.792077
707.632435	60826.465484	32.797095
708.437357	60938.602177	32.802112
709.099525	61047.780142	32.807130
710.092412	61162.623492	32.812148
711.045902	61253.243800	32.817165
712.096142	61354.882994	32.822183
712.185766	61462.046915	32.827200
713.243729	61551.355731	32.832218
714.038656	61664.749444	32.837236
714.775604	61773.419699	32.842253
715.546945	61866.822027	32.847271
715.835795	61982.538373	32.852288
716.595527	62089.696069	32.857306
717.178213	62189.299433	32.862324
718.129465	62296.673077	32.867341
718.580236	62402.031639	32.872359
718.945748	62505.394998	32.877376
719.437018	62620.190394	32.882394
720.133415	62755.265952	32.887412
720.935109	62860.385645	32.892429
721.903315	62967.734747	32.897447
722.513040	63090.634884	32.902464
723.036873	63212.494432	32.907482
724.068089	63309.128124	32.912500
724.544590	63418.298920	32.917517
725.837036	63522.310739	32.922535
726.491225	63631.845205	32.927552
727.319777	63723.552687	32.932570
728.239728	63819.663596	32.937588
728.804218	63912.471072	32.942605
729.562970	64020.574525	32.947623
730.278402	64116.632110	32.952640
730.745605	64212.851230	32.957658
731.605608	64317.330386	32.962676
732.075948	64425.622655	32.967693
732.835016	64533.273656	32.972711
733.379500	64628.546476	32.977728
734.145839	64743.131363	32.982746
735.025892	64858.589361	32.987764
735.316449	64971.465262	32.992781
736.430665	65084.875791	32.997799
737.036147	65202.764076	33.002816
737.693874	65304.772192	33.007834
738.467581	65426.489827	33.012852
739.004745	65543.139756	33.017869
740.170528	65656.633408	33.022887
740.599958	65793.473427	33.027904
741.466149	65899.716876	33.032922
742.100058	66019.741705	33.037940
742.832745	66141.331249	33.042957
743.935880	66252.392158	33.047975
744.589833	66378.427366	33.052992
745.447980	66493.209073	33.058010
746.202152	66614.311088	33.063028
746.686680	66730.818349	33.068045
747.449352	66846.098204	33.073063
748.030135	66973.767416	33.078080
748.885496	67090.398778	33.083098
749.660077	67220.174201	33.088116
750.034603	67352.298624	33.093133
751.369376	67469.725334	33.098151
751.879814	67590.898557	33.103168
752.761544	67718.876647	33.108186
753.785406	67838.335495	33.113204
754.475813	67949.739124	33.118221
755.164241	68066.068439	33.123239
755.836971	68201.221425	33.128256
756.606142	68313.296751	33.133274
757.344192	68443.534654	33.138292
758.200228	68571.079649	33.143309
758.995496	68693.780082	33.148327
759.348341	68828.035286	33.153344
760.007583	68957.701428	33.158362
761.007588	69082.943447	33.163380
761.512250	69217.568041	33.168397
762.511025	69340.523138	33.173415
763.107816	69462.457891	33.178432
764.046672	69595.546417	33.183450
765.216056	69721.023472	33.188468
765.929096	69842.277368	33.193485
767.135506	69960.542149	33.198503
767.736371	70089.150057	33.203520
768.651124	70197.038497	33.208538
769.792022	70323.750405	33.213556
770.223499	70437.928653	33.218573
771.194336	70550.109009	33.223591
771.969132	70657.308442	33.228608
772.782666	70761.258466	33.233626
773.485675	70884.309304	33.238644
773.998300	70994.120764	33.243661
775.427611	71100.974089	33.248679
775.757437	71218.423239	33.253696
776.473361	71327.855092	33.258714
777.272795	71423.243173	33.263732
777.563658	71538.044893	33.268749
778.595153	71647.799331	33.273767
778.973492	71762.897640	33.278784
779.550285	71879.664697	33.283802
780.164456	71987.713017	33.288820
780.534032	72127.310349	33.293837
781.503931	72236.047308	33.298855
782.404181	72376.614602	33.303872
782.930108	72503.656002	33.308890
784.008892	72631.068460	33.313908
784.551849	72760.998304	33.318925
785.655072	72883.286346	33.323943
786.760796	73007.085959	33.328960
787.515687	73128.225149	33.333978
788.052102	73256.711003	33.338996
788.831231	73382.798884	33.344013
789.800097	73513.693668	33.349031
790.510033	73652.334106	33.354048
791.201007	73778.527384	33.359066
792.162009	73884.023811	33.364084
793.213739	74025.607607	33.369101
793.753148	74155.198630	33.374119
794.407011	74279.156038	33.379136
795.202091	74420.228303	33.384154
796.330555	74562.561792	33.389172
797.057973	74687.584440	33.394189
797.927255	74807.752919	33.399207
798.783224	74939.288381	33.404224
799.353407	75067.956475	33.409242
800.254871	75204.127826	33.414260
801.135946	75335.623594	33.419277
801.982833	75464.602486	33.424295
802.454615	75603.282058	33.429312
803.284994	75750.232236	33.434330
804.172034	75876.405321	33.439348
804.665072	76017.025541	33.444365
805.470677	76157.462242	33.449383
806.208383	76304.146849	33.454400
806.944891	76462.589660	33.459418
808.093864	76590.652545	33.464436
808.754146	76728.542860	33.469453
809.661252	76860.100410	33.474471
810.218331	77015.743463	33.479488
811.033555	77175.949290	33.484506
812.339980	77298.361418	33.489524
812.433441	77443.136125	33.494541
813.495504	77596.049858	33.499559
814.438616	77747.782589	33.504576
814.936993	77882.455937	33.509594
815.804906	78035.151776	33.514612
816.702252	78191.822156	33.519629
817.776047	78327.168505	33.524647
818.438983	78482.583039	33.529664
819.031224	78642.703488	33.534682
820.088002	78781.901026	33.539700
820.315409	78942.191400	33.544717
821.530332	79091.978272	33.549735
822.510495	79244.069329	33.554752
822.898141	79390.294579	33.559770
824.141089	79545.892753	33.564788
825.173871	79696.662554	33.569805
825.785371	79824.440729	33.574823
826.873376	79977.625914	33.579840
827.648018	80123.975501	33.584858
828.723956	80270.782331	33.589876
829.909743	80416.572555	33.594893
830.629164	80536.740041	33.599911
831.358028	80659.917585	33.604928
831.766778	80794.642301	33.609946
832.987616	80924.388283	33.614964
833.497699	81068.997556	33.619981
834.359560	81206.831746	33.624999
835.454545	81346.652532	33.630016
836.084522	81462.614119	33.635034
837.149293	81602.068255	33.640052
837.650713	81753.496279	33.645069
838.396618	81890.980567	33.650087
839.496537	82029.141048	33.655104
839.849307	82176.592115	33.660122
840.822867	82304.172763	33.665140
841.601082	82472.393481	33.670157
842.315454	82613.044073	33.675175
843.227925	82766.928793	33.680192
843.953464	82918.163108	33.685210
845.231467	83063.797043	33.690228
845.738049	83215.784355	33.695245
846.556578	83360.154879	33.700263
847.098017	83514.238765	33.705280
847.953574	83672.409301	33.710298
848.862459	83829.857236	33.715316
849.554353	84005.904054	33.720333
850.645670	84159.711700	33.725351
851.382340	84325.238852	33.730368
852.252210	84491.017251	33.735386
853.012891	84649.033049	33.740404
853.833102	84820.895647	33.745421
854.638888	84975.186120	33.750439
855.607107	85144.274546	33.755456
856.379091	85313.086599	33.760474
857.641040	85459.883581	33.765492
858.883107	85622.394601	33.770509
859.619641	85776.651254	33.775527
861.003441	85929.720139	33.780544
862.153847	86083.904177	33.785562
863.524218	86229.460693	33.790580
864.262154	86372.813135	33.795597
864.998806	86519.077184	33.800615
865.641912	86666.566103	33.805632
866.533153	86805.226398	33.810650
867.523328	86952.552260	33.815668
868.266443	87106.766048	33.820685
869.172644	87260.219949	33.825703
869.787363	87411.951304	33.830720
870.556317	87561.342319	33.835738
871.494119	87711.187302	33.840756
872.198214	87871.006107	33.845773
873.012903	88025.112896	33.850791
873.749348	88179.537344	33.855808
874.353406	88343.685016	33.860826
875.490079	88505.689380	33.865844
876.212463	88675.185751	33.870861
877.260837	88817.964072	33.875879
878.453727	88977.716029	33.880896
879.328545	89128.795409	33.885914
880.518391	89272.983235	33.890932
881.312037	89436.759186	33.895949
882.261095	89580.317880	33.900967
883.068977	89732.639809	33.905984
883.564358	89889.551568	33.911002
884.761675	90036.501871	33.916020
885.563317	90188.840420	33.921037
886.208873	90348.635056	33.926055
886.841981	90500.680691	33.931072
887.796036	90661.976922	33.936090
888.934297	90820.370759	33.941108
889.519298	90973.490519	33.946125
890.453651	91112.795566	33.951143
891.442699	91269.774143	33.956160
892.179827	91420.504803	33.961178
893.105067	91573.641846	33.966196
893.819750	91723.840196	33.971213
894.620408	91887.207836	33.976231
895.641649	92035.939911	33.981248
896.260634	92210.009892	33.986266
897.085415	92365.231739	33.991284
898.197305	92531.381330	33.996301
898.818756	92699.809154	34.001319
899.910937	92847.496604	34.006336
900.725963	93013.280825	34.011354
901.532865	93187.453419	34.016372
902.501834	93354.284160	34.021389
903.463767	93519.838742	34.026407
904.762860	93686.655243	34.031424
905.710201	93845.879026	34.036442
906.198279	94008.053134	34.041460
907.370442	94191.951242	34.046477
907.949155	94351.992384	34.051495
909.110915	94519.843637	34.056512
909.978023	94694.434839	34.061530
910.985787	94857.978228	34.066548
911.639053	95038.588492	34.071565
912.636357	95223.289113	34.076583
913.547549	95384.282189	34.081600
914.060819	95576.167141	34.086618
915.003364	95755.260130	34.091636
916.086618	95932.774091	34.096653
916.580087	96114.342794	34.101671
917.741890	96293.701003	34.106688
918.803671	96483.413643	34.111706
919.739029	96672.401689	34.116724
920.658042	96853.209286	34.121741
921.217711	97045.800643	34.126759
922.552135	97227.808386	34.131776
923.559973	97423.449385	34.136794
924.431172	97605.131254	34.141812
925.913856	97784.029504	34.146829
926.516800	97963.371810	34.151847
927.517317	98133.262001	34.156864
928.221741	98319.800275	34.161882
929.486133	98507.614845	34.166900
930.569350	98683.667219	34.171917
931.315019	98871.089053	34.176935
932.835577	99045.394201	34.181952
933.361126	99220.396605	34.186970
934.672217	99400.233701	34.191988
935.323624	99580.788740	34.197005
935.967587	99762.682073	34.202023
937.098662	99935.747259	34.207040
938.038437	100129.375847	34.212058
938.465369	100315.651899	34.217076
939.764325	100491.731965	34.222093
940.697182	100675.420123	34.227111
941.783898	100863.623493	34.232128
942.555066	101045.625345	34.237146
943.294401	101225.823083	34.242164
944.706556	101406.651751	34.247181
945.663494	101601.061141	34.252199
946.745305	101771.089067	34.257216
947.795836	101954.918993	34.262234
948.215135	102124.260920	34.267252
949.361258	102315.092684	34.272269
950.339583	102505.858604	34.277287
951.167963	102675.516519	34.282304
952.260893	102828.841116	34.287322
953.159243	102998.850508	34.292340
954.019404	103175.401448	34.297357
954.839883	103355.860388	34.302375
955.593154	103524.428283	34.307392
956.955205	103707.883763	34.312410
957.934581	103877.967891	34.317428
959.403811	104040.627464	34.322445
959.715503	104224.525956	34.327463
961.154970	104394.290580	34.332480
962.164143	104558.973230	34.337498
963.035603	104730.036879	34.342516
964.145968	104906.488678	34.347533
964.490986	105083.384629	34.352551
965.741855	105263.133605	34.357568
966.682448	105440.414884	34.362586
967.322881	105624.838881	34.367604
968.241024	105813.612845	34.372621
968.974415	106016.501486	34.377639
970.563163	106187.462597	34.382656
970.962810	106376.668158	34.387674
971.923419	106566.668994	34.392692
973.073859	106747.077969	34.397709
973.380176	106963.963003	34.402727
974.578850	107163.554137	34.407744
975.497912	107361.115873	34.412762
976.526823	107565.512795	34.417780
977.448332	107767.649281	34.422797
978.462316	107966.048430	34.427815
979.086417	108168.807012	34.432832
980.363056	108379.172719	34.437850
981.220077	108599.159258	34.442868
982.318152	108798.057353	34.447885
983.072327	109018.026325	34.452903
983.839704	109232.358582	34.457920
985.037520	109444.455598	34.462938
985.652449	109663.325580	34.467956
987.186013	109880.069749	34.472973
987.896330	110098.104216	34.477991
989.036090	110308.849673	34.483008
990.305074	110527.821366	34.488026
991.515663	110732.199827	34.493044
992.663677	110941.555528	34.498061
993.865469	111167.877542	34.503079
994.676113	111362.395978	34.508096
995.717209	111582.161167	34.513114
996.443176	111793.239827	34.518132
997.755433	111987.502580	34.523149
998.488558	112204.840857	34.528167
999.316048	112431.640524	34.533184
1000.470617	112630.760178	34.538202
1001.468268	112853.760326	34.543220
1002.538166	113073.368072	34.548237
1003.586902	113287.103193	34.553255
1004.434946	113495.805934	34.558272
1005.321115	113714.385020	34.563290
1006.475621	113942.156604	34.568308
1007.675864	114152.313670	34.573325
1008.129909	114367.840208	34.578343
1009.603691	114584.542925	34.583360
1010.577447	114796.351153	34.588378
1011.708671	115027.049250	34.593396
1012.978738	115236.987632	34.598413
1013.699642	115452.833241	34.603431
1014.681320	115656.133248	34.608448
1015.990127	115870.719487	34.613466
1016.798528	116095.233878	34.618484
1017.887704	116288.461454	34.623501
1019.204365	116489.989194	34.628519
1019.991347	116688.172419	34.633536
1021.223720	116891.465322	34.638554
1021.899871	117088.529405	34.643572
1022.706722	117278.617650	34.648589
1023.528362	117497.097602	34.653607
1024.918235	117701.637300	34.658624
1025.970931	117907.222392	34.663642
1026.633289	118121.691740	34.668660
1028.086263	118323.830867	34.673677
1028.529327	118541.025636	34.678695
1029.712426	118767.412557	34.683712
1030.478301	118974.801197	34.688730
1031.268024	119209.213562	34.693748
1032.275868	119424.573265	34.698765
1033.079974	119670.352543	34.703783
1034.044379	119888.877898	34.708800
1034.945516	120119.820161	34.713818
1036.115144	120364.936812	34.718836
1037.228695	120594.884807	34.723853
1038.217956	120840.314022	34.728871
1039.280981	121085.454366	34.733888
1040.731909	121312.957473	34.738906
1041.984034	121548.389535	34.743924
1043.180274	121773.898170	34.748941
1044.336374	122008.640183	34.753959
1045.817625	122236.741055	34.758976
1047.189055	122447.083135	34.763994
1048.100638	122673.646769	34.769012
1049.976617	122882.755523	34.774029
1051.006125	123097.999446	34.779047
1052.156832	123304.734503	34.784064
1053.658836	123507.370528	34.789082
1054.497282	123725.070981	34.794100
1055.227576	123931.208175	34.799117
1056.491835	124136.168806	34.804135
1057.242078	124358.323883	34.809152
1058.610189	124552.029525	34.814170
1059.311476	124776.147411	34.819188
1060.246376	124992.624611	34.824205
1061.100080	125207.494625	34.829223
1061.900061	125436.594358	34.834240
1062.789288	125659.458524	34.839258
1063.745376	125896.038570	34.844276
1064.611208	126122.344510	34.849293
1065.351436	126362.715199	34.854311
1066.051370	126610.128339	34.859328
1067.131751	126851.131130	34.864346
1068.063968	127104.023047	34.869364
1069.154562	127349.400594	34.874381
1070.386172	127603.539984	34.879399
1070.985546	127863.299134	34.884416
1072.424441	128105.672175	34.889434
1073.495707	128363.050942	34.894452
1074.225317	128621.755718	34.899469
1075.492874	128870.221497	34.904487
1076.640674	129128.544630	34.909504
1078.054473	129376.521381	34.914522
1079.189921	129638.982811	34.919540
1080.673645	129866.456588	34.924557
1082.362514	130120.097642	34.929575
1082.995621	130354.762782	34.934592
1084.669931	130595.988402	34.939610
1085.419451	130832.247679	34.944628
1086.315582	131072.743510	34.949645
1088.021043	131309.292225	34.954663
1088.807467	131535.422900	34.959680
1090.146359	131738.939131	34.964698
1091.191777	131960.073872	34.969716
1092.325579	132179.357558	34.974733
1093.661767	132397.937526	34.979751
1094.375207	132623.999313	34.984768
1095.686877	132829.022839	34.989786
1096.634919	133050.853109	34.994804
1097.694249	133274.022928	34.999821
1098.954790	133485.676203	35.004839
1099.713607	133712.790375	35.009856
1100.836835	133927.486264	35.014874
1101.795618	134161.758272	35.019892
1102.685959	134393.368473	35.024909
1103.696775	134629.904455	35.029927
1104.747171	134870.948659	35.034944
1106.205673	135099.947419	35.039962
1106.933482	135340.870897	35.044980
1108.219224	135576.442984	35.049997
1109.383623	135821.912499	35.055015
1109.963252	136073.261331	35.060032
1111.357156	136310.139333	35.065050
1112.251639	136553.795306	35.070068
1113.509764	136799.573642	35.075085
1114.632224	137059.600785	35.080103
1115.725796	137301.429186	35.085120
1117.011765	137560.064072	35.090138
1117.856117	137822.006814	35.095156
1119.113826	138070.900853	35.100173
1120.343048	138311.509818	35.105191
1120.966107	138571.162189	35.110208
1122.614099	138831.255967	35.115226
1123.621260	139088.249858	35.120244
1124.624058	139341.265318	35.125261
1126.144056	139601.449611	35.130279
1126.813704	139871.894086	35.135296
1127.947874	140120.608248	35.140314
1129.261008	140388.681101	35.145332
1130.021797	140655.870954	35.150349
1131.463680	140926.424625	35.155367
1132.218675	141183.945258	35.160384
1133.587466	141445.157700	35.165402
1135.060030	141719.224841	35.170420
1135.991141	141989.528918	35.175437
1137.017595	142256.547990	35.180455
1137.929572	142543.419455	35.185472
1139.199515	142796.860358	35.190490
1140.366933	143078.786941	35.195508
1141.346955	143364.335263	35.200525
1142.074025	143635.269214	35.205543
1143.365293	143911.704220	35.210560
1144.574179	144182.410734	35.215578
1145.642940	144474.243062	35.220596
1146.968593	144766.568011	35.225613
1148.658061	145044.024105	35.230631
1149.451843	145324.521493	35.235648
1150.177357	145590.816924	35.240666
1151.390280	145880.151635	35.245684
1152.550489	146177.740224	35.250701
1154.054060	146450.748883	35.255719
1154.708607	146748.400351	35.260736
1155.840586	147029.299237	35.265754
1157.396873	147316.369665	35.270772
1158.243093	147613.147010	35.275789
1159.636553	147895.277689	35.280807
1160.695593	148191.986627	35.285824
1162.005044	148479.690440	35.290842
1162.773015	148758.785948	35.295860
1164.127194	149048.300433	35.300877
1165.556292	149323.346956	35.305895
1166.206581	149594.617906	35.310912
1167.905438	149854.747379	35.315930
1169.170922	150132.312764	35.320948
1170.149687	150413.668976	35.325965
1171.597022	150676.838906	35.330983
1172.730854	150954.102450	35.336000
1173.988746	151212.957216	35.341018
1175.444531	151491.414566	35.346036
1176.550709	151754.242586	35.351053
1177.617079	152034.670748	35.356071
1178.484580	152316.757307	35.361088
1179.508622	152594.114574	35.366106
1180.858628	152875.986167	35.371124
1182.067090	153148.484630	35.376141
1183.524973	153423.328431	35.381159
1184.516135	153713.535304	35.386176
1185.540958	154000.301483	35.391194
1186.879958	154282.553175	35.396212
1187.494376	154575.974435	35.401229
1188.663439	154861.188476	35.406247
1189.043961	155168.034732	35.411264
1190.608655	155473.939586	35.416282
1191.952747	155789.117615	35.421300
1192.948699	156104.216137	35.426317
1193.782828	156401.280846	35.431335
1194.950976	156722.508040	35.436352
1196.358012	157042.632902	35.441370
1197.235883	157354.830767	35.446388
1198.558585	157682.839488	35.451405
1200.015659	157992.676153	35.456423
1201.146383	158335.424178	35.461440
1202.499344	158653.071992	35.466458
1204.357779	158946.016233	35.471476
1205.405727	159277.914498	35.476493
1207.369299	159584.495826	35.481511
1208.433969	159901.617574	35.486528
1209.612402	160201.432080	35.491546
1210.773772	160515.307759	35.496564
1212.034121	160838.937858	35.501581
1213.171180	161138.182538	35.506599
1214.067766	161453.694923	35.511616
1215.229023	161769.166047	35.516634
1217.081450	162086.974009	35.521652
1218.505812	162401.924459	35.526669
1220.362073	162679.519743	35.531687
1222.034627	162977.839381	35.536704
1223.240581	163268.714841	35.541722
1224.671839	163561.382062	35.546740
1225.926752	163848.092136	35.551757
1227.144178	164133.046837	35.556775
1228.230277	164435.178293	35.561792
1229.166317	164717.303373	35.566810
1230.400451	165014.428404	35.571828
1231.670760	165311.397288	35.576845
1232.748710	165592.388243	35.581863
1233.399331	165902.988488	35.586880
1234.062756	166213.398547	35.591898
1235.751652	166523.527393	35.596916
1236.610957	166844.262953	35.601933
1237.868200	167148.263103	35.606951
1239.058363	167457.859228	35.611968
1239.992800	167775.315703	35.616986
1241.602501	168096.951675	35.622004
1242.369330	168421.507879	35.627021
1243.320413	168732.142141	35.632039
1244.786489	169074.706914	35.637056
1245.641199	169394.586331	35.642074
1247.001922	169709.550097	35.647092
1248.206563	170029.718899	35.652109
1249.064545	170345.962864	35.657127
1250.163824	170661.953505	35.662144
1251.539785	170975.515127	35.667162
1253.030873	171299.566594	35.672180
1254.339954	171631.936532	35.677197
1255.998779	171945.014012	35.682215
1257.147431	172256.198270	35.687232
1258.572502	172583.733947	35.692250
1259.702132	172889.418333	35.697268
1260.785441	173223.232875	35.702285
1262.347565	173535.880256	35.707303
1262.984877	173874.328718	35.712320
1264.603447	174208.455336	35.717338
1265.835977	174535.313153	35.722356
1266.660938	174879.270748	35.727373
1268.370502	175209.683881	35.732391
1269.258162	175544.460854	35.737408
1270.569699	175886.492610	35.742426
1271.907036	176239.563333	35.747444
1273.207740	176586.919198	35.752461
1274.894278	176919.111885	35.757479
1275.867770	177262.186352	35.762496
1277.369459	177601.444919	35.767514
1278.758117	177939.912264	35.772532
1279.986383	178300.516298	35.777549
1281.256822	178646.952632	35.782567
1282.509223	178995.539183	35.787584
1283.433316	179333.458151	35.792602
1285.001511	179691.515958	35.797620
1286.188266	180044.537265	35.802637
1287.610997	180399.958885	35.807655
1288.449245	180766.610098	35.812672
1289.748509	181112.741349	35.817690
1291.630483	181463.969752	35.822708
1292.876652	181830.751632	35.827725
1294.706958	182174.162446	35.832743
1296.355993	182510.688227	35.837760
1297.881942	182864.053706	35.842778
1299.117494	183210.679105	35.847796
1300.556017	183556.689438	35.852813
1301.712475	183889.637250	35.857831
1303.293904	184229.650234	35.862848
1304.538292	184569.556007	35.867866
1306.132431	184898.642784	35.872884
1307.266727	185253.104225	35.877901
1308.561453	185582.231896	35.882919
1309.683653	185940.101522	35.887936
1310.875780	186267.841352	35.892954
1312.211298	186615.043420	35.897972
1313.306076	186968.608625	35.902989
1314.498629	187318.021942	35.908007
1315.694320	187672.184255	35.913024
1316.724500	188024.065923	35.918042
1318.209810	188370.784579	35.923060
1319.355641	188740.612979	35.928077
1320.450694	189116.887873	35.933095
1321.953498	189471.010794	35.938112
1323.096362	189834.893409	35.943130
1324.115672	190198.836796	35.948148
1325.634458	190573.185293	35.953165
1326.970442	190936.192462	35.958183
1328.485826	191301.393757	35.963200
1329.266536	191705.689923	35.968218
1330.809599	192059.948901	35.973236
1332.127655	192439.064698	35.978253
1333.322792	192810.154877	35.983271
1335.217561	193165.898402	35.988288
1336.378962	193524.469014	35.993306
1337.668933	193873.499488	35.998324
1338.773256	194232.274108	36.003341
1340.351548	194580.156581	36.008359
1341.737966	194943.560501	36.013376
1342.931427	195302.491666	36.018394
1344.361559	195649.071610	36.023412
1345.720275	196013.425770	36.028429
1346.625364	196388.330460	36.033447
1348.251360	196747.033446	36.038464
1349.216685	197117.501832	36.043482
1350.239443	197489.410158	36.048500
1351.703633	197870.667851	36.053517
1353.011746	198254.035617	36.058535
1354.216579	198640.926681	36.063552
1355.089881	199027.303426	36.068570
1356.798414	199416.566192	36.073588
1357.810275	199821.244758	36.078605
1359.548991	200203.346643	36.083623
1361.360331	200591.240798	36.088640
1362.334793	200988.873542	36.093658
1364.520219	201370.768622	36.098676
1366.165820	201757.693754	36.103693
1367.645064	202142.185416	36.108711
1369.416252	202508.970336	36.113728
1370.816181	202895.713798	36.118746
1372.318087	203274.735754	36.123764
1373.344818	203656.555222	36.128781
1374.958512	204038.508401	36.133799
1376.808710	204417.618599	36.138816
1377.949093	204798.714348	36.143834
1379.488127	205165.716264	36.148852
1380.573875	205544.983867	36.153869
1381.992526	205928.553543	36.158887
1383.847360	206305.971321	36.163904
1384.943440	206689.102947	36.168922
1386.007735	207064.191746	36.173940
1387.204777	207454.954283	36.178957
1388.825755	207842.372945	36.183975
1390.109412	208231.753824	36.188992
1391.512274	208628.265640	36.194010
1392.925177	209007.534593	36.199028
1394.544623	209402.084547	36.204045
1395.385735	209791.431898	36.209063
1396.994468	210190.355497	36.214080
1398.142503	210578.957633	36.219098
1399.535983	210974.936641	36.224116
1400.805439	211369.388885	36.229133
1402.578856	211778.095811	36.234151
1403.783395	212186.695451	36.239168
1404.867962	212587.901206	36.244186
1406.318808	212989.937281	36.249204
1407.915062	213399.163815	36.254221
1409.269093	213809.727482	36.259239
1410.974249	214216.273272	36.264256
1411.915086	214621.575653	36.269274
1413.501992	215021.820890	36.274292
1414.741604	215428.601450	36.279309
1416.524836	215843.294208	36.284327
1418.537284	216249.112815	36.289344
1419.693199	216651.976095	36.294362
1420.654347	217056.371712	36.299380
1422.386498	217474.889842	36.304397
1423.664745	217879.033490	36.309415
1425.220250	218287.450709	36.314432
1426.139561	218714.718244	36.319450
1427.446541	219101.109197	36.324468
1428.754602	219523.693694	36.329485
1429.758194	219948.666864	36.334503
1431.342555	220388.175394	36.339520
1432.297758	220794.924171	36.344538
1434.163874	221203.987897	36.349556
1435.360257	221615.271842	36.354573
1436.659327	222036.217350	36.359591
1437.933772	222453.866760	36.364608
1439.126987	222873.385325	36.369626
1440.815837	223291.909369	36.374644
1442.383997	223727.345308	36.379661
1443.673073	224158.053976	36.384679
1445.161304	224585.251742	36.389696
1446.675005	225020.066724	36.394714
1448.121516	225446.563428	36.399732
1449.576097	225873.288965	36.404749
1451.192963	226315.330655	36.409767
1452.884734	226728.837738	36.414784
1454.461341	227172.718023	36.419802
1455.741533	227613.372251	36.424820
1456.973261	228038.262653	36.429837
1458.459043	228488.233257	36.434855
1459.870166	228934.331550	36.439872
1461.257823	229383.076891	36.444890
1462.874372	229824.089701	36.449908
1464.766202	230268.208209	36.454925
1465.931696	230720.220602	36.459943
1467.647896	231164.193231	36.464960
1469.185995	231610.685943	36.469978
1470.757607	232056.361721	36.474996
1472.420974	232498.137423	36.480013
1473.184363	232945.016158	36.485031
1474.898063	233404.008117	36.490048
1476.745681	233866.205321	36.495066
1478.171255	234305.180722	36.500084
1479.520190	234753.187446	36.505101
1481.380985	235216.199348	36.510119
1482.820148	235662.872882	36.515136
1484.448276	236109.364050	36.520154
1485.480801	236570.179538	36.525172
1487.144672	237024.414702	36.530189
1488.816210	237477.100298	36.535207
1490.443888	237934.950841	36.540224
1491.645057	238388.554631	36.545242
1493.169270	238854.349919	36.550260
1495.410688	239312.153438	36.555277
1496.590781	239746.534775	36.560295
1498.544554	240207.512322	36.565312
1499.789596	240649.149905	36.570330
1501.371056	241096.727832	36.575348
1502.639322	241557.973963	36.580365
1503.906060	242021.736163	36.585383
1505.379168	242471.494041	36.590400
1506.697991	242946.070953	36.595418
1508.049297	243411.295408	36.600436
1510.318055	243856.022048	36.605453
1511.873323	244305.287266	36.610471
1514.024768	244747.164398	36.615488
1515.484564	245211.129637	36.620506
1516.753172	245651.528218	36.625524
1518.303187	246113.397121	36.630541
1519.911523	246558.593000	36.635559
1521.146194	247000.752089	36.640576
1523.000974	247450.023899	36.645594
1524.455108	247905.840185	36.650612
1526.097817	248345.800041	36.655629
1527.300775	248814.639896	36.660647
1528.874087	249253.901108	36.665664
1530.536651	249694.545296	36.670682
1531.601783	250131.833782	36.675700
1533.389594	250551.500860	36.680717
1534.811453	250987.969346	36.685735
1536.273043	251410.333041	36.690752
1537.991884	251850.132005	36.695770
1539.226425	252291.814917	36.700788
1540.958442	252719.850886	36.705805
1541.974855	253156.794772	36.710823
1543.182648	253604.224337	36.715840
1544.562644	254069.357251	36.720858
1546.144696	254519.164456	36.725876
1547.791794	254970.764863	36.730893
1549.195781	255445.370183	36.735911
1550.677526	255899.233921	36.740928
1552.108601	256371.015553	36.745946
1553.640548	256849.004578	36.750964
1555.326748	257307.839701	36.755981
1556.691242	257802.495903	36.760999
1558.676145	258266.489753	36.766016
1560.114182	258750.667972	36.771034
1561.668934	259223.649593	36.776052
1563.419580	259699.139303	36.781069
1564.720594	260183.899255	36.786087
1566.433568	260671.715872	36.791104
1567.835597	261163.927762	36.796122
1569.188923	261660.008963	36.801140
1570.931139	262135.728702	36.806157
1572.516592	262634.946875	36.811175
1573.879959	263138.418519	36.816192
1575.479009	263647.185815	36.821210
1576.704589	264150.425826	36.826228
1578.242501	264657.018127	36.831245
1579.937063	265177.251281	36.836263
1581.397642	265670.620722	36.841280
1583.377077	266184.480864	36.846298
1584.986970	266708.181855	36.851316
1586.719820	267212.098484	36.856333
1588.226104	267724.714568	36.861351
1589.757655	268241.314323	36.866368
1591.730753	268756.189533	36.871386
1592.914922	269274.014129	36.876404
1594.938173	269782.707041	36.881421
1596.367991	270299.473839	36.886439
1598.295924	270811.534481	36.891456
1600.443572	271328.460995	36.896474
1601.814374	271833.118360	36.901492
1603.478725	272339.098355	36.906509
1604.976335	272867.688266	36.911527
1606.517376	273373.433054	36.916544
1608.427339	273886.508386	36.921562
1609.829739	274393.112709	36.926580
1612.023260	274894.200277	36.931597
1613.553538	275387.292960	36.936615
1615.454322	275913.626436	36.941632
1617.582972	276403.062200	36.946650
1618.788646	276912.412464	36.951668
1620.720273	277397.204777	36.956685
1622.256162	277905.202999	36.961703
1623.242927	278411.360157	36.966720
1625.028569	278920.559684	36.971738
1626.389133	279442.935733	36.976756
1627.885623	279930.918986	36.981773
1629.175571	280447.944391	36.986791
1630.811783	280964.708161	36.991808
1632.219313	281482.422806	36.996826
1633.404197	282003.271854	37.001844
1635.194215	282515.002001	37.006861
1636.387132	283028.175556	37.011879
1637.819484	283549.487512	37.016896
1639.724414	284074.123797	37.021914
1641.239072	284590.745209	37.026932
1642.936593	285104.261315	37.031949
1644.383155	285620.713007	37.036967
1645.983862	286141.786080	37.041984
1647.643078	286667.877249	37.047002
1648.980969	287198.287063	37.052020
1650.923078	287734.158195	37.057037
1652.366381	288276.053543	37.062055
1653.281840	288811.734583	37.067072
1655.230639	289355.879425	37.072090
1656.697557	289907.213877	37.077108
1658.585960	290453.269504	37.082125
1660.096846	291023.414074	37.087143
1661.246306	291579.569470	37.092160
1663.310134	292126.935594	37.097178
1664.846461	292717.642859	37.102196
1666.744670	293284.157680	37.107213
1668.454437	293850.548632	37.112231
1669.987420	294426.237065	37.117248
1671.739027	295005.569644	37.122266
1673.035595	295587.336633	37.127284
1675.067417	296162.451785	37.132301
1677.113835	296752.547230	37.137319
1678.801182	297320.347597	37.142336
1680.214593	297900.686582	37.147354
1681.698589	298505.596963	37.152372
1684.254696	299075.937205	37.157389
1685.726343	299653.920489	37.162407
1687.355892	300248.891501	37.167424
1689.504759	300835.925335	37.172442
1691.529974	301415.280541	37.177460
1693.202227	302001.471901	37.182477
1694.923943	302583.410185	37.187495
1696.735599	303159.691868	37.192512
1698.476709	303742.178741	37.197530
1699.823871	304324.117493	37.202548
1701.921243	304909.662257	37.207565
1703.660733	305489.497216	37.212583
1704.870363	306076.222274	37.217600
1706.862819	306664.236581	37.222618
1708.239223	307261.999327	37.227636
1710.098962	307844.567406	37.232653
1711.655294	308444.755811	37.237671
1713.099216	309047.041027	37.242688
1714.856391	309634.515273	37.247706
1716.678692	310253.363706	37.252724
1717.992185	310868.177362	37.257741
1719.845246	311473.196360	37.262759
1721.433893	312076.222820	37.267776
1723.398603	312690.051688	37.272794
1725.077105	313318.017039	37.277812
1727.007003	313914.065734	37.282829
1728.605788	314524.283658	37.287847
1730.433328	315149.187516	37.292864
1732.382182	315754.969951	37.297882
1733.520688	316363.547457	37.302900
1735.376946	316993.941464	37.307917
1737.201697	317611.333850	37.312935
1738.377964	318236.293453	37.317952
1740.460329	318866.303599	37.322970
1741.759248	319489.606735	37.327988
1743.734051	320131.075261	37.333005
1745.474372	320768.513744	37.338023
1747.054477	321401.122836	37.343040
1748.815167	322015.109520	37.348058
1750.311633	322631.774836	37.353076
1752.099080	323248.183253	37.358093
1753.862235	323870.759848	37.363111
1755.711766	324485.775169	37.368128
1757.175982	325091.732982	37.373146
1759.045565	325707.241010	37.378164
1761.068533	326331.299498	37.383181
1763.028876	326955.235106	37.388199
1764.653274	327571.679159	37.393216
1766.751719	328177.019893	37.398234
1768.647328	328793.102146	37.403252
1770.723420	329410.316171	37.408269
1772.967112	330026.099775	37.413287
1774.541922	330638.331389	37.418304
1776.113995	331269.013991	37.423322
1777.638611	331891.040388	37.428340
1779.611712	332500.673221	37.433357
1781.045927	333129.428667	37.438375
1782.684250	333764.693203	37.443392
1784.783713	334392.690085	37.448410
1786.112454	335032.129201	37.453428
1788.153609	335682.232333	37.458445
1789.690822	336322.180458	37.463463
1791.236897	336970.826668	37.468480
1792.858113	337626.661937	37.473498
1794.647159	338283.882950	37.478516
1796.384780	338939.505023	37.483533
1798.204145	339613.610277	37.488551
1799.619033	340279.219182	37.493568
1801.333791	340949.592808	37.498586
1803.006777	341630.752242	37.503604
1805.017290	342312.024473	37.508621
1806.637216	343010.789459	37.513639
1808.278924	343702.154870	37.518656
1810.112719	344385.280634	37.523674
1811.959031	345079.689385	37.528692
1814.052618	345771.864623	37.533709
1816.313953	346462.783935	37.538727
1817.948224	347157.755939	37.543744
1820.044254	347848.479265	37.548762
1822.126224	348535.311678	37.553780
1823.546846	349240.109801	37.558797
1825.840026	349933.129833	37.563815
1827.719340	350616.132487	37.568832
1829.873421	351301.668066	37.573850
1831.791033	351991.267217	37.578868
1833.743649	352682.245682	37.583885
1836.242640	353350.639567	37.588903
1837.769384	354044.306141	37.593920
1839.931310	354722.047788	37.598938
1841.927148	355398.029957	37.603956
1843.506088	356077.825784	37.608973
1845.671599	356747.744814	37.613991
1847.235058	357430.744181	37.619008
1849.211819	358110.035851	37.624026
1851.137528	358786.939816	37.629044
1853.353713	359454.701311	37.634061
1855.500837	360114.090441	37.639079
1857.407050	360779.293558	37.644096
1859.451542	361449.309005	37.649114
1860.890400	362120.402734	37.654132
1862.616756	362795.547921	37.659149
1864.715964	363445.198967	37.664167
1866.302961	364115.752682	37.669184
1868.231111	364794.001820	37.674202
1870.254883	365456.875076	37.679220
1871.686699	366131.783358	37.684237
1873.577029	366797.953633	37.689255
1875.079058	367443.679157	37.694272
1876.845039	368094.601282	37.699290
1878.520307	368771.858149	37.704308
1880.229336	369417.363730	37.709325
1882.201499	370075.700775	37.714343
1883.840418	370752.750271	37.719360
1885.768239	371417.234693	37.724378
1887.493568	372089.197743	37.729396
1889.201165	372763.129782	37.734413
1891.336797	373439.210736	37.739431
1892.941629	374115.163682	37.744448
1894.711087	374806.928516	37.749466
1896.723699	375501.936938	37.754484
1898.157981	376192.817069	37.759501
1899.933570	376885.783081	37.764519
1901.473509	377611.413630	37.769536
1903.683095	378318.811369	37.774554
1905.528791	379028.993526	37.779572
1907.750500	379745.895279	37.784589
1909.812426	380453.552429	37.789607
1911.744099	381170.243841	37.794624
1914.003069	381870.966826	37.799642
1916.131240	382597.535657	37.804660
1917.394449	383323.977778	37.809677
1919.672875	384041.463382	37.814695
1921.660661	384770.873020	37.819712
1923.484027	385498.113038	37.824730
1925.090603	386218.095908	37.829748
1927.045985	386951.620217	37.834765
1929.321407	387695.799426	37.839783
1931.392575	388442.226061	37.844800
1933.420007	389170.541113	37.849818
1935.336766	389898.857669	37.854836
1936.895246	390639.815815	37.859853
1939.072125	391380.933284	37.864871
1941.410699	392128.648025	37.869888
1943.056896	392876.154709	37.874906
1944.911700	393625.763438	37.879924
1946.624871	394374.312559	37.884941
1948.522156	395132.216669	37.889959
1950.247712	395918.188623	37.894976
1952.025493	396675.769500	37.899994
1954.059032	397435.240579	37.905012
1955.949748	398214.661926	37.910029
1957.829521	398975.512859	37.915047
1959.704650	399753.375470	37.920064
1961.443165	400539.831015	37.925082
1963.669593	401327.806686	37.930100
1965.487029	402123.227925	37.935117
1967.804153	402884.588612	37.940135
1969.533789	403698.327066	37.945152
1971.064300	404496.668975	37.950170
1973.044854	405295.091477	37.955188
1974.721082	406105.906199	37.960205
1976.809156	406912.930302	37.965223
1978.380312	407723.157890	37.970240
1980.423151	408538.908367	37.975258
1982.304587	409364.212367	37.980276
1984.168602	410184.630231	37.985293
1986.078931	411005.978340	37.990311
1987.753079	411843.983708	37.995328
1990.279924	412672.120375	38.000346
1992.005275	413508.950647	38.005364
1993.668178	414340.065654	38.010381
1995.955186	415190.276335	38.015399
1998.070382	416026.633312	38.020416
2000.250571	416854.696071	38.025434
2002.789032	417687.105519	38.030452
2004.480141	418505.040258	38.035469
2006.653444	419296.227558	38.040487
2008.953294	420107.325012	38.045504
2011.048180	420899.615128	38.050522
2013.165418	421699.524208	38.055540
2015.061232	422496.988200	38.060557
2017.482326	423281.629051	38.065575
2019.441398	424087.134640	38.070592
2021.272015	424882.254333	38.075610
2023.683695	425685.379870	38.080628
2025.445211	426482.155686	38.085645
2027.691481	427282.572513	38.090663
2029.788932	428083.747046	38.095680
2031.357433	428897.842457	38.100698
2033.679526	429705.508135	38.105716
2035.661433	430517.050377	38.110733
2037.725049	431324.147154	38.115751
2039.764340	432160.480950	38.120768
2041.619712	432965.025014	38.125786
2043.168076	433786.701781	38.130804
2045.214798	434639.549598	38.135821
2047.369317	435469.115509	38.140839
2049.341792	436308.146683	38.145856
2051.298126	437150.034935	38.150874
2053.521428	437988.811642	38.155892
2055.534119	438837.511652	38.160909
2058.613482	439663.686346	38.165927
2060.708886	440508.615873	38.170944
2062.887870	441344.593734	38.175962
2064.944935	442181.319550	38.180980
2066.860883	443023.147816	38.185997
2068.901156	443863.203351	38.191015
2071.202764	444724.889409	38.196032
2072.881542	445582.445151	38.201050
2075.195621	446410.165201	38.206068
2077.088945	447281.683362	38.211085
2078.887668	448134.667008	38.216103
2081.186964	448982.779350	38.221120
2082.964130	449854.465755	38.226138
2085.453993	450703.389113	38.231156
2087.575870	451581.978965	38.236173
2089.688068	452435.700430	38.241191
2092.059408	453305.225313	38.246208
2093.832826	454178.808087	38.251226
2096.564758	455023.471808	38.256244
2098.533722	455888.151330	38.261261
2100.671434	456750.137446	38.266279
2102.825402	457614.056885	38.271296
2104.851319	458490.146727	38.276314
2107.603157	459347.119058	38.281332
2109.220907	460207.376937	38.286349
2111.581171	461066.464716	38.291367
2113.885440	461934.978772	38.296384
2115.770794	462807.821262	38.301402
2118.295736	463659.643096	38.306420
2120.144310	464531.506333	38.311437
2122.377188	465391.895124	38.316455
2124.624356	466253.002189	38.321472
2126.465031	467130.362201	38.326490
2128.658759	467985.185456	38.331508
2130.388933	468847.324898	38.336525
2132.394255	469728.027786	38.341543
2134.545987	470589.262111	38.346560
2136.261095	471469.680610	38.351578
2138.453523	472356.902166	38.356596
2140.171626	473250.173122	38.361613
2142.274854	474139.448312	38.366631
2144.263186	475032.388588	38.371648
2146.050060	475906.880737	38.376666
2147.829160	476777.191108	38.381684
2150.189930	477659.387104	38.386701
2152.178951	478542.360192	38.391719
2154.339136	479418.343309	38.396736
2155.943148	480313.720251	38.401754
2158.067432	481201.442741	38.406772
2160.054235	482102.376030	38.411789
2162.237288	483005.454306	38.416807
2164.075675	483923.440701	38.421824
2165.808528	484851.244002	38.426842
2168.367880	485805.320189	38.431860
2170.278504	486731.482212	38.436877
2171.934106	487658.445929	38.441895
2174.680771	488616.581494	38.446912
2176.492486	489565.833864	38.451930
2178.700315	490511.486793	38.456948
2180.753472	491477.455350	38.461965
2182.926097	492442.694595	38.466983
2185.400812	493418.681161	38.472000
2187.282689	494406.468938	38.477018
2189.779544	495366.192654	38.482036
2191.663942	496357.551662	38.487053
2193.679942	497332.634672	38.492071
2196.402846	498318.796494	38.497088
2198.680007	499320.412442	38.502106
2200.786325	500313.773974	38.507124
2202.814696	501304.970862	38.512141
2205.610078	502302.287774	38.517159
2208.174211	503295.144377	38.522176
2210.327513	504296.028581	38.527194
2212.663360	505284.919747	38.532212
2215.220021	506288.844011	38.537229
2217.618844	507296.010445	38.542247
2219.869542	508271.069440	38.547264
2221.766798	509272.195703	38.552282
2224.261713	510263.783700	38.557300
2226.814955	511277.231311	38.562317
2229.081373	512266.515056	38.567335
2231.359286	513258.508032	38.572352
2233.387619	514259.250734	38.577370
2236.048821	515255.743261	38.582388
2238.283109	516257.988633	38.587405
2240.512448	517251.704394	38.592423
2242.709531	518255.289605	38.597440
2244.929540	519256.639635	38.602458
2247.173113	520253.739114	38.607476
2249.813540	521256.452410	38.612493
2251.933017	522254.047568	38.617511
2254.399615	523254.643869	38.622528
2256.303001	524270.278483	38.627546
2258.900943	525273.440644	38.632564
2260.817754	526276.296093	38.637581
2262.865012	527292.862705	38.642599
2265.475026	528302.872146	38.647616
2267.202057	529308.678765	38.652634
2269.678557	530326.479221	38.657652
2271.816207	531349.048916	38.662669
2274.193340	532363.352483	38.667687
2276.965003	533372.184923	38.672704
2278.937507	534398.094153	38.677722
2281.413010	535399.335366	38.682740
2283.988506	536417.603938	38.687757
2286.338619	537433.573433	38.692775
2288.601561	538450.291062	38.697792
2290.763672	539478.577603	38.702810
2292.935694	540488.674604	38.707828
2295.114581	541490.699188	38.712845
2297.202368	542485.977004	38.717863
2299.374592	543462.456981	38.722880
2301.777900	544452.362920	38.727898
2304.151780	545435.463952	38.732916
2306.360362	546425.514482	38.737933
2308.257368	547429.527550	38.742951
2310.254865	548431.691555	38.747968
2312.264688	549444.693020	38.752986
2314.301873	550445.749315	38.758004
2316.393088	551473.119777	38.763021
2318.859781	552503.971139	38.768039
2321.243822	553526.111923	38.773056
2323.120530	554558.363187	38.778074
2325.907892	555586.415059	38.783092
2328.529760	556636.429338	38.788109
2330.732921	557683.164235	38.793127
2333.058023	558729.093879	38.798144
2335.350558	559785.750146	38.803162
2337.756657	560840.545376	38.808180
2339.931554	561903.182387	38.813197
2342.083198	562982.013893	38.818215
2344.350454	564050.541178	38.823232
2346.837933	565138.382814	38.828250
2349.147154	566211.950415	38.833268
2351.542086	567300.782162	38.838285
2353.522017	568398.579260	38.843303
2356.319384	569493.989373	38.848320
2358.348580	570588.027211	38.853338
2360.437939	571686.329356	38.858356
2363.161344	572805.816405	38.863373
2365.314263	573920.480644	38.868391
2367.928502	575018.860612	38.873408
2370.152657	576142.150628	38.878426
2372.670844	577268.352897	38.883444
2375.001929	578387.159451	38.888461
2377.061029	579521.914906	38.893479
2379.602825	580654.681435	38.898496
2381.531605	581794.819213	38.903514
2384.091564	582950.095512	38.908532
2386.528604	584100.619601	38.913549
2388.779082	585245.650694	38.918567
2391.307399	586387.419897	38.923584
2393.611394	587551.430031	38.928602
2396.218753	588725.505423	38.933620
2398.786215	589871.051047	38.938637
2400.918692	591036.057080	38.943655
2403.459517	592207.548285	38.948672
2405.189055	593381.714342	38.953690
2407.765075	594554.773208	38.958708
2410.278539	595728.928805	38.963725
2412.545206	596910.422871	38.968743
2415.229110	598090.176674	38.973760
2417.871504	599281.088356	38.978778
2420.641816	600454.178356	38.983796
2423.337852	601631.869644	38.988813
2426.038191	602809.290385	38.993831
2428.402510	603991.202648	38.998848
2430.479830	605160.325047	39.003866
2433.009260	606334.059231	39.008884
2435.941618	607505.153876	39.013901
2438.375707	608683.567078	39.018919
2441.060047	609852.558908	39.023936
2443.497594	611026.223984	39.028954
2446.025357	612180.890088	39.033972
2448.701946	613353.472297	39.038989
2450.919896	614537.561966	39.044007
2453.380672	615687.375185	39.049024
2456.036603	616832.386198	39.054042
2458.076038	617984.381092	39.059060
2460.917228	619103.223426	39.064077
2463.109712	620240.406957	39.069095
2465.818349	621350.942711	39.074112
2467.921182	622493.355613	39.079130
2470.472012	623629.127367	39.084148
2472.749334	624754.230698	39.089165
2475.087425	625904.641091	39.094183
2477.022182	627041.604846	39.099200
2479.333997	628195.671605	39.104218
2481.654115	629367.046033	39.109236
2484.048203	630530.937315	39.114253
2486.174112	631710.876510	39.119271
2488.713656	632874.586510	39.124288
2491.134279	634078.232169	39.129306
2493.221817	635271.959767	39.134324
2495.536967	636474.000140	39.139341
2497.958739	637689.910241	39.144359
2500.103966	638909.716465	39.149376
2502.639593	640139.644494	39.154394
2505.070308	641374.981841	39.159412
2507.654879	642620.871888	39.164429
2509.362712	643864.660074	39.169447
2512.185275	645130.009395	39.174464
2514.554692	646396.473156	39.179482
2516.941286	647668.111639	39.184500
2519.877367	648925.289998	39.189517
2522.161253	650233.268362	39.194535
2524.772809	651519.439199	39.199552
2526.926685	652823.412474	39.204570
2529.176746	654121.767614	39.209588
2531.968023	655427.337809	39.214605
2534.704940	656745.349118	39.219623
2537.312089	658045.621727	39.224640
2540.141535	659361.424456	39.229658
2542.600263	660687.868179	39.234676
2544.941138	662009.619865	39.239693
2547.394102	663329.729587	39.244711
2550.099305	664659.573666	39.249728
2552.807245	665999.636461	39.254746
2555.504977	667333.542366	39.259764
2558.468285	668674.035696	39.264781
2560.963394	670008.248807	39.269799
2563.682890	671335.422835	39.274816
2566.367775	672661.471739	39.279834
2568.909049	674012.919577	39.284852
2572.211667	675335.009493	39.289869
2574.328396	676669.835844	39.294887
2576.886519	678005.442701	39.299904
2579.922580	679340.978038	39.304922
2582.334997	680672.647134	39.309940
2585.403253	682007.295755	39.314957
2587.798926	683346.035066	39.319975
2590.591833	684663.352938	39.324992
2593.827426	685987.063459	39.330010
2596.220211	687309.379937	39.335028
2598.972941	688632.586687	39.340045
2601.457072	689961.005973	39.345063
2604.209473	691279.555940	39.350080
2607.015114	692587.928249	39.355098
2609.265675	693905.778243	39.360116
2611.981200	695230.055282	39.365133
2614.605558	696562.980573	39.370151
2617.043875	697889.833874	39.375168
2619.766726	699194.868294	39.380186
2622.111192	700530.614066	39.385204
2624.668152	701856.057399	39.390221
2626.930490	703178.374408	39.395239
2629.367155	704471.666197	39.400256
2631.936371	705789.670333	39.405274
2633.813870	707098.718983	39.410292
2636.639359	708393.244471	39.415309
2638.866045	709720.663109	39.420327
2641.125330	711039.154651	39.425344
2644.107616	712361.780449	39.430362
2646.311344	713706.707915	39.435380
2648.640072	715040.759021	39.440397
2651.273882	716398.999925	39.445415
2653.556979	717758.069844	39.450432
2656.130054	719125.778546	39.455450
2658.235737	720498.139818	39.460468
2661.050344	721889.597443	39.465485
2663.217141	723298.337005	39.470503
2665.747531	724706.579814	39.475520
2668.277353	726116.263841	39.480538
2670.676973	727551.332012	39.485556
2673.275256	728980.779498	39.490573
2675.856234	730427.619867	39.495591
2678.528576	731871.125692	39.500608
2681.705014	733333.209667	39.505626
2684.026809	734799.368258	39.510644
2687.081609	736260.844177	39.515661
2689.760124	737739.394703	39.520679
2692.274495	739220.907789	39.525696
2695.087664	740685.664108	39.530714
2697.982632	742185.463829	39.535732
2700.871132	743675.707168	39.540749
2703.638966	745163.075481	39.545767
2706.647637	746647.065993	39.550784
2709.423857	748133.476504	39.555802
2712.575796	749637.583414	39.560820
2715.329839	751110.269949	39.565837
2718.191996	752608.823382	39.570855
2720.870477	754103.865585	39.575872
2724.050392	755597.402549	39.580890
2726.298102	757090.261244	39.585908
2729.462220	758569.827774	39.590925
2732.172837	760078.126567	39.595943
2735.168781	761576.088621	39.600960
2738.026320	763058.572987	39.605978
2740.847665	764559.811219	39.610996
2743.432154	766038.557078	39.616013
2746.419567	767553.483118	39.621031
2749.059728	769046.624660	39.626048
2752.129245	770544.852665	39.631066
2755.022379	772043.888721	39.636084
2757.761642	773522.107453	39.641101
2760.495914	775032.994821	39.646119
2762.930314	776526.872383	39.651136
2765.948192	778016.420718	39.656154
2768.793886	779534.316825	39.661172
2771.607542	781026.671331	39.666189
2774.478360	782536.278624	39.671207
2777.528263	784020.321299	39.676224
2780.538147	785519.174065	39.681242
2783.312648	787023.736310	39.686260
2786.299494	788499.114564	39.691277
2789.045545	789999.916487	39.696295
2791.875611	791486.712678	39.701312
2795.112605	792972.345797	39.706330
2797.357202	794484.972638	39.711348
2799.686136	795964.245731	39.716365
2802.593180	797466.373999	39.721383
2805.104818	798984.059690	39.726400
2808.026323	800487.885665	39.731418
2810.424865	801968.763517	39.736436
2813.176143	803447.651877	39.741453
2815.924593	804925.734661	39.746471
2818.284815	806403.074810	39.751488
2821.217916	807865.674823	39.756506
2823.405707	809357.418121	39.761524
2826.395286	810840.393518	39.766541
2829.000227	812326.089459	39.771559
2831.174005	813837.864224	39.776576
2834.061283	815347.522093	39.781594
2836.594517	816877.996063	39.786612
2839.335931	818402.911160	39.791629
2842.004458	819935.056244	39.796647
2844.921034	821470.614559	39.801664
2847.795752	823033.976187	39.806682
2850.462968	824601.246368	39.811700
2853.276125	826179.482632	39.816717
2855.768541	827759.684318	39.821735
2858.441822	829344.885545	39.826752
2861.609294	830929.230692	39.831770
2864.096159	832527.576888	39.836788
2866.745972	834138.750620	39.841805
2869.837133	835761.915855	39.846823
2871.906553	837398.082000	39.851840
2875.470182	839012.559755	39.856858
2877.733207	840660.709898	39.861876
2881.249664	842302.098353	39.866893
2883.761892	843963.167398	39.871911
2886.485764	845622.307359	39.876928
2889.343797	847273.114838	39.881946
2892.533551	848947.925521	39.886964
2895.576390	850627.073758	39.891981
2898.499404	852293.551357	39.896999
2901.669510	853968.476097	39.902016
2904.792001	855645.480565	39.907034
2907.887283	857326.305035	39.912052
2911.041225	858998.995914	39.917069
2914.203607	860678.213882	39.922087
2917.281856	862352.911825	39.927104
2920.518380	864018.398243	39.932122
2923.331403	865677.682560	39.937140
2926.616515	867372.383067	39.942157
2929.308791	869049.075215	39.947175
2931.907864	870728.607995	39.952192
2935.225122	872399.709890	39.957210
2938.306821	874082.288035	39.962228
2941.217605	875770.708260	39.967245
2944.243361	877431.350440	39.972263
2947.490067	879112.378334	39.977280
2950.668169	880785.977239	39.982298
2953.780748	882479.986569	39.987316
2956.655435	884146.683880	39.992333
2959.844694	885822.319571	39.997351
2962.597885	887491.267406	40.002368
2965.270567	889161.678727	40.007386
2968.029290	890854.659001	40.012404
2970.982878	892538.329438	40.017421
2973.980952	894225.935404	40.022439
2976.530785	895929.123843	40.027456
2979.439097	897623.550583	40.032474
2982.537370	899321.006206	40.037492
2985.179677	901027.180182	40.042509
2988.003527	902727.992876	40.047527
2990.610224	904449.316061	40.052544
2994.091814	906145.711279	40.057562
2996.719230	907874.254817	40.062580
2999.537809	909608.578796	40.067597
3002.665526	911338.751752	40.072615
3005.295990	913054.237842	40.077632
3008.199844	914746.561072	40.082650
3011.091443	916443.264566	40.087668
3013.361547	918153.758804	40.092685
3016.553344	919842.442424	40.097703
3019.364036	921545.637646	40.102720
3022.429592	923261.592985	40.107738
3025.584434	924987.156180	40.112756
3028.446924	926707.228243	40.117773
3031.853999	928416.210600	40.122791
3034.473021	930147.583929	40.127808
3038.095261	931878.612892	40.132826
3041.159655	933598.443931	40.137844
3044.427347	935327.256427	40.142861
3047.757080	937062.095946	40.147879
3050.462508	938804.693932	40.152896
3053.665694	940537.640616	40.157914
3056.797626	942276.525683	40.162932
3059.755726	944025.467752	40.167949
3062.645655	945779.564418	40.172967
3065.527549	947547.585371	40.177984
3068.869733	949315.306180	40.183002
3072.040116	951077.961254	40.188020
3074.831251	952843.316183	40.193037
3078.301658	954631.316571	40.198055
3081.007100	956464.285895	40.203072
3083.899455	958289.802576	40.208090
3086.658492	960138.131457	40.213108
3089.300160	962004.946728	40.218125
3092.517330	963856.796775	40.223143
3095.483235	965736.712033	40.228160
3098.281274	967605.201824	40.233178
3101.166656	969498.351686	40.238196
3104.052196	971404.733865	40.243213
3107.349655	973307.488213	40.248231
3110.482251	975214.123778	40.253248
3113.149673	977135.018692	40.258266
3116.163755	979061.351039	40.263284
3119.179353	981006.030475	40.268301
3122.644118	982941.501324	40.273319
3124.907161	984896.178604	40.278336
3128.046107	986866.293563	40.283354
3130.754553	988841.343203	40.288372
3133.923225	990831.483345	40.293389
3136.809028	992815.432172	40.298407
3139.958749	994813.416251	40.303424
3142.818986	996815.213388	40.308442
3145.921683	998826.460723	40.313460
3148.871333	1000846.727000	40.318477
3152.198797	1002870.964997	40.323495
3154.907439	1004911.556701	40.328512
3158.283183	1006935.882607	40.333530
3161.331341	1008978.730164	40.338548
3164.339123	1011041.872188	40.343565
3167.643775	1013083.867407	40.348583
3171.084749	1015149.694619	40.353600
3174.424442	1017180.610011	40.358618
3177.694271	1019245.249787	40.363636
3180.854411	1021301.700005	40.368653
3184.116015	1023349.160376	40.373671
3187.298792	1025405.164095	40.378688
3190.748967	1027469.450489	40.383706
3194.147329	1029521.875838	40.388724
3197.324229	1031576.190091	40.393741
3200.377074	1033633.628820	40.398759
3203.390522	1035702.374198	40.403776
3207.082967	1037744.682089	40.408794
3210.584978	1039792.345045	40.413812
3213.821887	1041832.743909	40.418829
3217.044576	1043826.443015	40.423847
3220.187375	1045823.098095	40.428864
3222.956407	1047819.095304	40.433882
3225.874720	1049816.080499	40.438900
3228.904340	1051825.024386	40.443917
3232.002052	1053828.995542	40.448935
3234.884377	1055847.366686	40.453952
3237.808233	1057866.145458	40.458970
3241.096572	1059898.052747	40.463988
3243.799042	1061946.302169	40.469005
3247.042030	1063990.532215	40.474023
3249.858327	1066056.523973	40.479040
3253.076782	1068118.027164	40.484058
3256.165119	1070210.991204	40.489076
3258.892600	1072305.419313	40.494093
3262.386184	1074408.308343	40.499111
3265.435372	1076519.655133	40.504128
3268.355541	1078633.078799	40.509146
3271.666361	1080769.637977	40.514164
3274.657020	1082912.108065	40.519181
3277.795264	1085066.714544	40.524199
3281.063114	1087229.430464	40.529216
3283.964451	1089409.593914	40.534234
3287.396907	1091601.209311	40.539252
3290.356961	1093793.734957	40.544269
3293.879314	1095987.666079	40.549287
3297.138030	1098203.166308	40.554304
3300.260553	1100420.831870	40.559322
3303.813458	1102626.364879	40.564340
3306.749995	1104863.773954	40.569357
3310.020481	1107089.152572	40.574375
3313.453269	1109319.771461	40.579392
3316.756037	1111575.461585	40.584410
3320.251990	1113821.232280	40.589428
3323.453951	1116078.755211	40.594445
3327.423675	1118323.892293	40.599463
3330.813133	1120591.075217	40.604480
3334.023158	1122833.969226	40.609498
3337.820576	1125078.671836	40.614516
3340.891202	1127348.922856	40.619533
3344.594693	1129608.525002	40.624551
3348.102165	1131869.285552	40.629568
3351.252682	1134112.563001	40.634586
3355.192056	1136359.972002	40.639604
3358.438659	1138624.624368	40.644621
3361.960340	1140878.611902	40.649639
3365.236320	1143139.530834	40.654656
3368.373485	1145399.316911	40.659674
3371.908922	1147650.604799	40.664692
3374.799822	1149916.341504	40.669709
3378.633981	1152188.219539	40.674727
3381.735608	1154462.729939	40.679744
3384.807808	1156726.544246	40.684762
3388.191787	1159008.286181	40.689780
3391.079513	1161296.564149	40.694797
3394.798532	1163591.526371	40.699815
3398.055525	1165863.332705	40.704832
3401.252975	1168156.378144	40.709850
3404.593004	1170440.019027	40.714868
3408.361470	1172734.534677	40.719885
3411.797790	1175022.360003	40.724903
3415.021831	1177314.947047	40.729920
3418.500737	1179626.676161	40.734938
3422.650833	1181909.381129	40.739956
3426.294928	1184213.594209	40.744973
3429.412989	1186507.301216	40.749991
3433.008497	1188788.286547	40.755008
3436.578437	1191052.420366	40.760013
3440.073019	1193250.368059	40.765018
3443.369333	1195408.732367	40.770023
3446.566277	1197493.761434	40.775028
3449.830392	1199498.104829	40.780032
3452.856709	1201438.316174	40.785037
3456.047651	1203291.809852	40.790042
3458.871531	1205074.509071	40.795047
3461.778404	1206758.403907	40.800052
3464.482589	1208393.270458	40.805056
3466.593430	1209937.653540	40.810061
3469.390268	1211401.906086	40.815066
3471.634808	1212795.563258	40.820071
3473.969137	1214133.730333	40.825076
3476.058607	1215396.399532	40.830080
3477.684285	1216589.085430	40.835085
3479.642373	1217718.529471	40.840090
3481.625890	1218796.412431	40.845095
3483.742048	1219804.248838	40.850100
3485.492324	1220755.988250	40.855104
3487.022121	1221648.555828	40.860109
3488.816624	1222483.303546	40.865114
3490.139279	1223263.462387	40.870119
3491.774607	1224014.882132	40.875124
3493.367383	1224695.348166	40.880128
3494.894812	1225330.559868	40.885133
3496.074024	1225903.782439	40.890138
3497.355422	1226455.367879	40.895143
3498.482947	1226964.278556	40.900148
3499.540936	1227425.102236	40.905152
3500.217054	1227851.337008	40.910157
3501.410515	1228237.153360	40.915162
3502.703152	1228608.839558	40.920167
3503.580715	1228937.010648	40.925172
3504.556463	1229216.554358	40.930176
3505.619405	1229483.105370	40.935181
3506.610769	1229707.596638	40.940186
3507.171954	1229897.366377	40.945191
3507.709366	1230057.386955	40.950196
3508.290690	1230215.996566	40.955200
3509.065025	1230340.349506	40.960205
3509.837144	1230430.107487	40.965210
3510.403510	1230516.168183	40.970215
3511.208543	1230562.282195	40.975220
3511.710668	1230612.827835	40.980224
3512.331692	1230616.082200	40.985229
3512.592357	1230594.314977	40.990234
3513.149408	1230575.389238	40.995239
3513.245786	1230533.229593	41.000244
3513.928887	1230478.758548	41.005248
3513.972831	1230414.601860	41.010253
3514.668716	1230329.637146	41.015258
3515.191845	1230232.857418	41.020263
3515.582125	1230112.879333	41.025268
3515.763559	1230005.987639	41.030272
3516.243644	1229872.001736	41.035277
3516.516183	1229717.717137	41.040282
3516.860836	1229561.830597	41.045287
3517.220931	1229375.347426	41.050292
3517.238876	1229202.343702	41.055296
3517.390835	1229026.887067	41.060301
3517.558608	1228820.269488	41.065306
3517.772046	1228627.254001	41.070311
3517.651543	1228409.101132	41.075316
3518.267245	1228193.989223	41.080320
3518.508615	1227973.705818	41.085325
3518.954967	1227746.195739	41.090330
3518.491636	1227509.495806	41.095335
3518.617204	1227257.200175	41.100340
3518.816086	1227019.155404	41.105344
3518.943504	1226776.165901	41.110349
3519.007021	1226508.260751	41.115354
3519.252891	1226245.163958	41.120359
3519.093619	1225987.252994	41.125364
3519.542621	1225709.256642	41.130368
3519.597829	1225427.763269	41.135373
3519.855665	1225153.407948	41.140378
3519.674980	1224863.801737	41.145383
3519.990955	1224574.003864	41.150388
3520.302210	1224275.975079	41.155392
3519.938603	1223982.427846	41.160397
3520.319320	1223694.342956	41.165402
3520.225135	1223384.284552	41.170407
3520.352123	1223083.041532	41.175412
3520.435044	1222762.177744	41.180416
3520.358834	1222462.518901	41.185421
3520.624760	1222137.943462	41.190426
3520.672210	1221825.992185	41.195431
3520.484693	1221508.456170	41.200436
3520.918679	1221187.435185	41.205440
3520.692554	1220868.184157	41.210445
3520.781671	1220534.006962	41.215450
3520.734267	1220215.246063	41.220455
3520.848097	1219878.966352	41.225460
3521.143815	1219549.829427	41.230464
3520.749185	1219219.196317	41.235469
3520.794617	1218879.217395	41.240474
3520.627554	1218541.493797	41.245479
3521.122077	1218211.863820	41.250484
3521.186746	1217866.299656	41.255488
3520.806354	1217534.059229	41.260493
3521.023732	1217186.180322	41.265498
3520.772383	1216846.582038	41.270503
3521.020186	1216495.472307	41.275508
3521.108322	1216147.076294	41.280512
3520.683946	1215802.294250	41.285517
3521.212747	1215439.376815	41.290522
3521.132206	1215101.130405	41.295527
3520.831059	1214748.307395	41.300532
3521.175075	1214398.346872	41.305536
3520.964060	1214052.943768	41.310541
3521.205421	1213693.597659	41.315546
3520.995699	1213357.034339	41.320551
3521.219903	1213001.758769	41.325556
3521.092392	1212648.949167	41.330560
3521.018616	1212297.509954	41.335565
3521.125626	1211924.774015	41.340570
3521.386882	1211585.021785	41.345575
3521.022867	1211225.040192	41.350580
3521.409846	1210865.939168	41.355584
3521.031246	1210498.608007	41.360589
3521.248337	1210134.803280	41.365594
3521.025312	1209774.228243	41.370599
3520.669430	1209424.510350	41.375604
3521.292149	1209053.446313	41.380608
3520.826391	1208703.978167	41.385613
3520.878219	1208331.738516	41.390618
3520.614974	1207979.752757	41.395623
3520.547410	1207621.529050	41.400628
3520.604080	1207268.786116	41.405632
3520.493812	1206912.767851	41.410637
3520.827448	1206556.932776	41.415642
3520.800358	1206208.065120	41.420647
3520.580254	1205836.532064	41.425652
3520.985253	1205475.644491	41.430656
3520.638713	1205120.946129	41.435661
3520.762495	1204762.397302	41.440666
3520.758268	1204407.030913	41.445671
3520.420972	1204035.386630	41.450676
3520.937492	1203680.915163	41.455680
3520.450370	1203324.897220	41.460685
3520.515867	1202961.076510	41.465690
3520.124223	1202618.118038	41.470695
3520.019488	1202257.650540	41.475700
3520.450068	1201900.538848	41.480704
3520.570984	1201537.827098	41.485709
3520.463152	1201177.471841	41.490714
3520.411103	1200826.835624	41.495719
3520.237228	1200459.876060	41.500724
3519.983510	1200110.818633	41.505728
3519.947092	1199760.388471	41.510733
3520.137863	1199400.797487	41.515738
3520.035396	1199059.805221	41.520743
3519.905891	1198689.428414	41.525748
3519.837946	1198337.686804	41.530752
3519.414609	1197996.301559	41.535757
3519.770923	1197641.439760	41.540762
3519.739591	1197300.976090	41.545767
3519.703403	1196935.150031	41.550772
3519.846045	1196588.603908	41.555776
3519.875675	1196244.775226	41.560781
3519.850893	1195889.479985	41.565786
3519.930076	1195545.502596	41.570791
3519.545518	1195174.163786	41.575796
3519.479747	1194830.913659	41.580800
3519.297864	1194484.936718	41.585805
3519.432365	1194142.546764	41.590810
3519.855004	1193787.314620	41.595815
3519.202980	1193431.859322	41.600820
3519.383263	1193086.198472	41.605824
3519.307122	1192754.082736	41.610829
3519.467436	1192400.395115	41.615834
3519.398208	1192057.806393	41.620839
3519.054280	1191703.120650	41.625844
3519.141269	1191349.936823	41.630848
3519.068752	1191008.406471	41.635853
3518.940894	1190659.439110	41.640858
3519.262461	1190312.065709	41.645863
3519.043016	1189966.731663	41.650868
3519.291097	1189625.996923	41.655872
3519.158899	1189291.129961	41.660877
3518.670671	1188938.157937	41.665882
3518.535841	1188597.794473	41.670887
3518.521446	1188266.037912	41.675892
3518.608198	1187919.106425	41.680896
3518.407218	1187590.627918	41.685901
3518.789440	1187246.893553	41.690906
3518.947130	1186918.125221	41.695911
3518.630443	1186578.787274	41.700916
3518.735841	1186232.397915	41.705920
3518.602121	1185906.716955	41.710925
3519.019673	1185557.221252	41.715930
3518.604939	1185209.061917	41.720935
3518.467543	1184865.066834	41.725940
3518.834765	1184528.680390	41.730944
3518.346390	1184197.870023	41.735949
3518.548658	1183849.329502	41.740954
3518.378077	1183509.484042	41.745959
3518.323160	1183180.889830	41.750964
3518.393721	1182841.807827	41.755968
3518.123819	1182513.394937	41.760973
3517.963413	1182174.495569	41.765978
3518.140555	1181848.320016	41.770983
3517.904343	1181522.850976	41.775988
3518.031017	1181174.331363	41.780992
3517.865540	1180857.187474	41.785997
3517.830927	1180519.100721	41.791002
3517.926852	1180203.756919	41.796007
3517.836073	1179874.865013	41.801012
3518.193707	1179529.116020	41.806016
3517.747304	1179203.441970	41.811021
3517.849923	1178873.701398	41.816026
3517.989369	1178549.020032	41.821031
3517.597427	1178218.377433	41.826036
3517.442015	1177887.298035	41.831040
3517.541727	1177576.033117	41.836045
3517.675729	1177258.620133	41.841050
3517.467272	1176937.569674	41.846055
3517.029994	1176605.607105	41.851060
3517.510817	1176281.293227	41.856064
3517.353389	1175967.995582	41.861069
3517.487559	1175636.913673	41.866074
3517.473569	1175321.574412	41.871079
3517.225215	1174999.468427	41.876084
3517.509418	1174670.091121	41.881088
3516.956909	1174344.884170	41.886093
3517.209408	1174035.078982	41.891098
3517.130581	1173723.424412	41.896103
3516.882873	1173397.071025	41.901108
3517.253365	1173085.492859	41.906112
3516.925926	1172782.120227	41.911117
3516.970920	1172455.282470	41.916122
3517.094832	1172141.708213	41.921127
3516.714782	1171830.367230	41.926132
3516.740089	1171500.643548	41.931136
3516.467177	1171205.941598	41.936141
3516.883561	1170879.792806	41.941146
3516.750397	1170575.222124	41.946151
3516.591630	1170261.675700	41.951156
3516.718468	1169958.063897	41.956160
3516.699856	1169649.080448	41.961165
3516.714130	1169332.147429	41.966170
3516.477175	1169023.540330	41.971175
3516.531636	1168717.697995	41.976180
3516.509760	1168415.625206	41.981184
3516.250823	1168100.738617	41.986189
3516.400321	1167793.222070	41.991194
3516.533991	1167487.766586	41.996199
3516.315280	1167184.239169	42.001204
3516.406684	1166877.716649	42.006208
3516.321750	1166567.145759	42.011213
3516.425647	1166255.109150	42.016218
3516.391599	1165965.264538	42.021223
3516.309782	1165674.184245	42.026228
3516.490985	1165349.711629	42.031232
3516.179497	1165036.915318	42.036237
3516.440018	1164725.422679	42.041242
3516.321362	1164414.257278	42.046247
3516.349436	1164108.810656	42.051252
3516.583040	1163791.316508	42.056256
3516.263233	1163495.053550	42.061261
3516.104410	1163177.681275	42.066266
3516.248967	1162876.016671	42.071271
3516.002157	1162584.319282	42.076276
3516.071568	1162271.861821	42.081280
3515.967246	1161967.445868	42.086285
3515.954193	1161658.555973	42.091290
3516.036220	1161360.027166	42.096295
3516.144720	1161058.358334	42.101300
3515.793910	1160755.424639	42.106304
3515.785464	1160460.167344	42.111309
3515.868084	1160162.704441	42.116314
3515.601930	1159847.322051	42.121319
3515.082429	1159555.595471	42.126324
3515.179772	1159265.925429	42.131328
3515.239907	1158990.426872	42.136333
3515.323366	1158691.367712	42.141338
3515.277295	1158404.699269	42.146343
3515.144802	1158121.055252	42.151348
3515.773359	1157829.043588	42.156352
3515.349475	1157541.633727	42.161357
3515.096101	1157235.359890	42.166362
3515.363831	1156956.126566	42.171367
3515.085575	1156666.942418	42.176372
3515.648158	1156359.726471	42.181376
3515.114839	1156065.064995	42.186381
3515.170078	1155778.993268	42.191386
3515.196590	1155502.749630	42.196391
3514.722996	1155212.476930	42.201396
3514.871860	1154922.937222	42.206400
3514.513266	1154644.251885	42.211405
3514.842074	1154365.060065	42.216410
3514.877804	1154091.863413	42.221415
3514.709014	1153806.951461	42.226420
3515.034393	1153520.523083	42.231424
3514.823170	1153243.632061	42.236429
3514.609821	1152964.076598	42.241434
3514.691899	1152680.198118	42.246439
3514.639220	1152391.120171	42.251444
3514.649252	1152114.985272	42.256448
3514.339413	1151846.840919	42.261453
3514.465915	1151564.030984	42.266458
3514.647600	1151282.995715	42.271463
3514.343688	1151003.256341	42.276468
3514.736576	1150727.080300	42.281472
3514.228294	1150463.538038	42.286477
3513.967329	1150172.383975	42.291482
3514.150580	1149908.605363	42.296487
3514.109346	1149631.306926	42.301492
3514.400173	1149358.296129	42.306496
3514.442277	1149084.933278	42.311501
3514.239761	1148814.817202	42.316506
3514.276957	1148540.384952	42.321511
3514.199829	1148259.894200	42.326516
3514.249175	1147991.589182	42.331520
3513.890562	1147736.507224	42.336525
3513.956987	1147464.572295	42.341530
3514.027488	1147196.602364	42.346535
3513.658636	1146923.668949	42.351540
3514.139611	1146660.910737	42.356544
3513.681314	1146391.660331	42.361549
3513.545492	1146125.186286	42.366554
3513.720170	1145861.964897	42.371559
3513.641577	1145600.383412	42.376564
3513.770006	1145326.432467	42.381568
3513.347898	1145075.308205	42.386573
3513.367173	1144814.619612	42.391578
3513.495468	1144551.340556	42.396583
3513.224522	1144299.206485	42.401588
3513.639230	1144035.759773	42.406592
3513.543057	1143783.477505	42.411597
3513.550558	1143519.692879	42.416602
3513.204922	1143252.160248	42.421607
3513.279650	1142999.053800	42.426612
3513.571819	1142744.287249	42.431616
3513.272236	1142502.503942	42.436621
3513.311634	1142223.759748	42.441626
3513.282471	1141983.141130	42.446631
3512.780872	1141723.903466	42.451636
3513.169154	1141471.051680	42.456640
3513.180324	1141231.151082	42.461645
3513.107572	1140971.521346	42.466650
3513.301418	1140711.645228	42.471655
3512.882207	1140466.942470	42.476660
3513.068123	1140218.428442	42.481664
3513.021654	1139974.590336	42.486669
3513.131221	1139705.664760	42.491674
3513.133310	1139459.897190	42.496679
3512.782791	1139210.570184	42.501684
3513.037271	1138957.620429	42.506688
3512.640607	1138706.569064	42.511693
3512.914713	1138460.520526	42.516698
3512.582977	1138205.638294	42.521703
3512.456687	1137972.826301	42.526708
3512.690663	1137719.536082	42.531712
3512.527222	1137473.988440	42.536717
3512.634701	1137230.473335	42.541722
3512.846964	1136985.220921	42.546727
3512.540267	1136753.904114	42.551732
3512.645268	1136510.546250	42.556736
3512.543488	1136259.900108	42.561741
3512.748404	1136014.983856	42.566746
3512.691827	1135776.651543	42.571751
3512.506213	1135527.408991	42.576756
3512.682291	1135272.207153	42.581760
3512.328456	1135043.292688	42.586765
3512.492869	1134798.896830	42.591770
3512.384040	1134546.176403	42.596775
3512.352973	1134312.048272	42.601780
3512.181545	1134079.262786	42.606784
3512.044136	1133844.656616	42.611789
3512.204141	1133603.341257	42.616794
3512.033647	1133371.759582	42.621799
3512.023902	1133134.440965	42.626804
3511.957265	1132895.980995	42.631808
3511.825101	1132667.497657	42.636813
3511.699838	1132420.379666	42.641818
3512.064193	1132206.712716	42.646823
3511.830299	1131976.981153	42.651828
3511.888858	1131739.874103	42.656832
3511.717287	1131515.814216	42.661837
3511.896809	1131290.071400	42.666842
3511.683807	1131067.615120	42.671847
3511.638413	1130844.076411	42.676852
3511.984522	1130610.293349	42.681856
3511.667139	1130380.791730	42.686861
3511.875181	1130142.258071	42.691866
3511.796268	1129908.989499	42.696871
3511.766071	1129694.811322	42.701876
3511.819456	1129474.050823	42.706880
3511.859593	1129241.303813	42.711885
3511.455760	1129006.052587	42.716890
3511.759308	1128778.851700	42.721895
3511.291139	1128557.663677	42.726900
3511.674943	1128318.448833	42.731904
3511.628021	1128100.500676	42.736909
3511.540927	1127883.881618	42.741914
3511.506528	1127656.117904	42.746919
3511.110751	1127432.874052	42.751924
3511.119486	1127213.358704	42.756928
3510.955815	1126995.004100	42.761933
3511.194131	1126782.566890	42.766938
3511.442411	1126559.941353	42.771943
3511.196485	1126334.058445	42.776948
3511.523722	1126115.777235	42.781952
3511.032660	1125901.807818	42.786957
3511.281909	1125680.001606	42.791962
3511.285319	1125458.416946	42.796967
3511.331579	1125252.705596	42.801972
3511.606604	1125036.006301	42.806977
3511.126163	1124807.908893	42.811981
3511.299288	1124577.790912	42.816986
3511.357965	1124359.482073	42.821991
3510.870792	1124159.906861	42.826996
3511.447104	1123933.882043	42.832001
3510.929587	1123706.029139	42.837005
3510.870178	1123492.938903	42.842010
3510.892575	1123298.196816	42.847015
3510.875197	1123071.471817	42.852020
3510.848743	1122858.826777	42.857025
3510.649958	1122648.867067	42.862029
3511.031819	1122446.609636	42.867034
3511.157549	1122225.822582	42.872039
3510.868215	1122018.613837	42.877044
3510.941293	1121780.775406	42.882049
3510.404146	1121577.113073	42.887053
3510.602428	1121388.365983	42.892058
3510.928197	1121171.977587	42.897063
3510.744547	1120948.903452	42.902068
3510.379832	1120736.515314	42.907073
3510.197657	1120539.992269	42.912077
3510.499583	1120332.906470	42.917082
3510.632462	1120137.269085	42.922087
3510.768020	1119927.433081	42.927092
3510.682519	1119717.244271	42.932097
3510.698493	1119520.460633	42.937101
3510.844582	1119300.882898	42.942106
3510.469716	1119084.906456	42.947111
3510.314137	1118893.557650	42.952116
3510.904843	1118689.218480	42.957121
3510.897432	1118482.397794	42.962125
3510.577256	1118270.571243	42.967130
3510.776869	1118055.601897	42.972135
3509.991146	1117856.983606	42.977140
3510.502714	1117651.188676	42.982145
3510.114759	1117444.581124	42.987149
3510.267713	1117232.921444	42.992154
3510.253301	1117043.579624	42.997159
3510.261263	1116836.692824	43.002164
3510.278001	1116628.938884	43.007169
3509.629428	1116432.532351	43.012173
3509.629484	1116244.494156	43.017178
3509.731621	1116046.043665	43.022183
3509.738026	1115866.378514	43.027188
3510.077358	1115659.201042	43.032193
3509.861433	1115465.737971	43.037197
3509.685614	1115276.932221	43.042202
3509.912979	1115097.109570	43.047207
3509.868843	1114896.543397	43.052212
3509.776872	1114703.032382	43.057217
3509.525534	1114506.966494	43.062221
3509.986783	1114319.833544	43.067226
3510.152895	1114141.228373	43.072231
3509.660295	1113943.370058	43.077236
3510.070219	1113743.067358	43.082241
3509.494956	1113553.027104	43.087245
3509.509222	1113363.741251	43.092250
3509.790745	1113166.298928	43.097255
3509.729407	1112980.349677	43.102260
3509.549020	1112777.533290	43.107265
3509.172922	1112605.642126	43.112269
3509.466766	1112434.016621	43.117274
3509.634699	1112244.475233	43.122279
3509.772120	1112055.695235	43.127284
3509.488201	1111860.587175	43.132289
3509.581083	1111686.300080	43.137293
3509.558815	1111499.053027	43.142298
3509.397890	1111303.713690	43.147303
3509.549808	1111121.099138	43.152308
3509.451183	1110929.170262	43.157313
3509.399785	1110751.060504	43.162317
3509.077324	1110564.307325	43.167322
3509.332032	1110386.230466	43.172327
3509.429552	1110199.681680	43.177332
3509.378315	1110013.150918	43.182337
3509.387787	1109839.962675	43.187341
3508.985137	1109656.626311	43.192346
3509.542266	1109469.117656	43.197351
3508.900683	1109296.496261	43.202356
3508.954056	1109114.688630	43.207361
3509.147998	1108941.345620	43.212365
3508.943682	1108759.091219	43.217370
3509.142017	1108569.606046	43.222375
3509.197453	1108402.663215	43.227380
3509.135300	1108216.644592	43.232385
3509.193967	1108041.863121	43.237389
3508.906987	1107865.796509	43.242394
3509.160868	1107695.839915	43.247399
3508.755432	1107523.599980	43.252404
3508.946974	1107338.845693	43.257409
3508.768467	1107164.265704	43.262413
3508.891501	1106980.274140	43.267418
3509.179970	1106815.153111	43.272423
3508.852110	1106644.113415	43.277428
3508.775285	1106466.916151	43.282433
3508.938760	1106290.341868	43.287437
3508.692387	1106107.049687	43.292442
3508.300928	1105943.732684	43.297447
3508.179527	1105779.124836	43.302452
3508.864892	1105598.144707	43.307457
3508.501393	1105436.622149	43.312461
3508.738942	1105264.586003	43.317466
3508.670817	1105104.628382	43.322471
3507.938891	1104948.213623	43.327476
3508.762048	1104767.469433	43.332481
3508.601873	1104600.444165	43.337485
3508.726101	1104436.232394	43.342490
3508.705576	1104272.517060	43.347495
3508.581605	1104102.318227	43.352500
3508.446647	1103919.984008	43.357505
3508.728142	1103763.463461	43.362509
3508.706361	1103591.512146	43.367514
3508.973982	1103424.284437	43.372519
3508.420194	1103258.333279	43.377524
3508.416015	1103092.095410	43.382529
3508.447049	1102926.802056	43.387533
3508.434422	1102758.644422	43.392538
3508.332601	1102583.998843	43.397543
3508.355181	1102425.953320	43.402548
3508.300898	1102272.502488	43.407553
3508.239547	1102102.612427	43.412557
3508.246262	1101933.279173	43.417562
3508.455270	1101766.869786	43.422567
3508.078937	1101619.569538	43.427572
3508.154220	1101450.687681	43.432577
3508.227370	1101292.887347	43.437581
3508.078522	1101134.545507	43.442586
3507.987960	1100985.364941	43.447591
3507.944193	1100825.467474	43.452596
3508.067198	1100657.221999	43.457601
3508.221776	1100506.554067	43.462605
3508.048873	1100347.046045	43.467610
3507.871931	1100189.732598	43.472615
3507.776453	1100036.224953	43.477620
3507.870641	1099888.417570	43.482625
3507.871644	1099720.545394	43.487629
3507.675748	1099565.128882	43.492634
3507.741482	1099416.930870	43.497639
3507.724489	1099265.204896	43.502644
3507.640217	1099114.346244	43.507649
3507.351290	1098964.473223	43.512653
3507.544460	1098817.480762	43.517658
3507.593224	1098668.500081	43.522663
3507.482483	1098527.000065	43.527668
3507.500420	1098375.338971	43.532673
3507.499850	1098232.091848	43.537677
3507.548217	1098079.461170	43.542682
3507.706094	1097931.972293	43.547687
3507.456431	1097787.702462	43.552692
3507.522775	1097637.925401	43.557697
3507.442751	1097493.715422	43.562701
3507.134404	1097351.356407	43.567706
3507.515995	1097208.019210	43.572711
3507.272496	1097064.876811	43.577716
3507.431012	1096906.934270	43.582721
3507.307696	1096773.042433	43.587725
3507.252286	1096631.770647	43.592730
3507.360772	1096490.755151	43.597735
3507.482238	1096342.176677	43.602740
3507.517928	1096199.922005	43.607745
3507.171485	1096055.430557	43.612749
3507.195115	1095919.675751	43.617754
3507.262669	1095771.664496	43.622759
3507.359439	1095635.316488	43.627764
3507.278605	1095492.009994	43.632769
3507.270844	1095358.351135	43.637773
3507.142601	1095213.609909	43.642778
3507.255641	1095060.787704	43.647783
3506.857426	1094932.923623	43.652788
3506.954989	1094794.066474	43.657793
3507.071215	1094667.163955	43.662797
3506.880180	1094524.998284	43.667802
3506.948683	1094383.073221	43.672807
3506.845911	1094257.632597	43.677812
3506.951558	1094117.321304	43.682817
3507.089646	1093985.422822	43.687821
3506.663404	1093852.274208	43.692826
3506.424382	1093710.860696	43.697831
3506.827340	1093589.436699	43.702836
3506.649865	1093463.032881	43.707841
3506.610918	1093323.969098	43.712845
3506.510537	1093186.730470	43.717850
3506.775419	1093057.660002	43.722855
3506.414078	1092932.805585	43.727860
3506.783505	1092810.508177	43.732865
3506.880083	1092685.572648	43.737869
3506.637190	1092550.351597	43.742874
3506.415532	1092410.432911	43.747879
3506.531036	1092292.473479	43.752884
3506.310267	1092162.983031	43.757889
3506.605562	1092056.189745	43.762893
3506.416203	1091914.433947	43.767898
3506.523878	1091796.560754	43.772903
3506.438631	1091669.429712	43.777908
3506.289849	1091542.401898	43.782913
3506.419015	1091415.516826	43.787917
3506.363002	1091302.638720	43.792922
3506.797172	1091177.421337	43.797927
3506.636565	1091055.554652	43.802932
3506.453557	1090920.857604	43.807937
3506.601573	1090796.157332	43.812941
3506.348875	1090674.488766	43.817946
3506.693782	1090538.641916	43.822951
3506.120353	1090423.436651	43.827956
3506.419625	1090289.027542	43.832961
3506.452565	1090176.781726	43.837965
3506.195169	1090056.345066	43.842970
3506.577965	1089927.851086	43.847975
3506.191121	1089809.920390	43.852980
3506.223273	1089677.934536	43.857985
3506.198208	1089556.107614	43.862989
3506.146485	1089433.132958	43.867994
3506.245412	1089303.329993	43.872999
3506.267205	1089196.525465	43.878004
3506.069955	1089074.907673	43.883009
3506.430787	1088966.605954	43.888013
3506.088790	1088849.413316	43.893018
3506.150581	1088733.684363	43.898023
3506.093876	1088604.848279	43.903028
3506.013566	1088490.191307	43.908033
3505.965595	1088372.652553	43.913037
3506.030413	1088260.840871	43.918042
3506.217236	1088143.737510	43.923047
3505.945140	1088032.168218	43.928052
3505.897405	1087910.020667	43.933057
3506.141120	1087795.678904	43.938061
3505.903500	1087671.449411	43.943066
3506.062500	1087556.924949	43.948071
3505.899817	1087454.236600	43.953076
3505.743209	1087338.418067	43.958081
3505.800695	1087228.886016	43.963085
3505.868140	1087110.151077	43.968090
3506.263872	1086998.354736	43.973095
3505.605518	1086893.437607	43.978100
3505.705730	1086768.556862	43.983105
3505.688930	1086658.738065	43.988109
3505.618633	1086550.171693	43.993114
3505.634733	1086437.276338	43.998119
3505.503392	1086338.778491	44.003124
3505.621425	1086227.778737	44.008129
3505.560574	1086126.486104	44.013133
3505.421540	1086027.217152	44.018138
3505.750024	1085913.301043	44.023143
3505.476931	1085800.631783	44.028148
3505.507753	1085700.753816	44.033153
3505.583785	1085584.380340	44.038157
3505.483635	1085476.564244	44.043162
3505.859002	1085379.595055	44.048167
3505.436235	1085274.895417	44.053172
3505.582817	1085169.045560	44.058177
3505.662218	1085067.518384	44.063181
3505.410433	1084970.645194	44.068186
3505.786006	1084850.468099	44.073191
3505.259154	1084747.788578	44.078196
3505.367408	1084638.195966	44.083201
3505.706887	1084537.383000	44.088205
3505.131015	1084437.677625	44.093210
3505.693126	1084335.769684	44.098215
3505.295778	1084233.442609	44.103220
3505.380968	1084120.200146	44.108225
3505.255779	1084028.083119	44.113229
3505.513496	1083922.286583	44.118234
3505.483662	1083821.425303	44.123239
3505.336870	1083721.156714	44.128244
3505.066587	1083600.962517	44.133249
3505.280148	1083504.178336	44.138253
3505.535247	1083418.700447	44.143258
3505.446379	1083311.127235	44.148263
3505.319532	1083217.270728	44.153268
3505.587054	1083119.511905	44.158273
3505.458665	1083009.350107	44.163277
3505.283318	1082913.098950	44.168282
3505.266482	1082790.255876	44.173287
3505.178545	1082699.261015	44.178292
3505.151754	1082607.199632	44.183297
3505.450286	1082505.300858	44.188301
3505.094269	1082413.290418	44.193306
3505.471456	1082314.540026	44.198311
3504.966120	1082220.153214	44.203316
3505.001542	1082111.672644	44.208321
3505.314926	1082023.573653	44.213325
3504.832190	1081924.382335	44.218330
3504.923218	1081832.384365	44.223335
3504.793113	1081751.643659	44.228340
3505.311242	1081646.047772	44.233345
3505.238046	1081546.782126	44.238349
3505.119063	1081463.253592	44.243354
3505.384813	1081358.365160	44.248359
3505.352375	1081260.142751	44.253364
3505.238681	1081150.612413	44.258369
3505.130809	1081057.770768	44.263373
3504.820481	1080967.838833	44.268378
3505.364554	1080856.947152	44.273383
3504.887692	1080766.847459	44.278388
3504.675227	1080669.603405	44.283393
3505.064453	1080589.239626	44.288397
3504.810209	1080498.715080	44.293402
3505.119387	1080406.848998	44.298407
3504.959642	1080310.837100	44.303412
3504.907123	1080210.008604	44.308417
3505.122306	1080126.788326	44.313421
3505.126799	1080035.733746	44.318426
3505.319584	1079922.674123	44.323431
3504.877971	1079838.694069	44.328436
3504.867238	1079738.329725	44.333441
3505.011239	1079650.124327	44.338445
3505.107345	1079556.647787	44.343450
3505.301933	1079455.572730	44.348455
3505.140574	1079382.286800	44.353460
3504.808613	1079283.598303	44.358465
3504.762894	1079179.007130	44.363469
3504.965979	1079091.550674	44.368474
3505.158591	1078998.048669	44.373479
3505.297722	1078917.221623	44.378484
3505.065568	1078809.583104	44.383489
3504.890639	1078718.919965	44.388493
3504.778311	1078641.009376	44.393498
3505.023028	1078536.262075	44.398503
3504.763219	1078444.360683	44.403508
3504.609141	1078350.232843	44.408513
3504.771319	1078255.091499	44.413517
3504.747641	1078173.032512	44.418522
3504.615314	1078083.887494	44.423527
3504.699197	1077991.921876	44.428532
3504.674936	1077908.131289	44.433537
3504.668943	1077820.208968	44.438541
3504.637421	1077728.449891	44.443546
3504.812134	1077647.022242	44.448551
3504.424574	1077565.206025	44.453556
3504.390764	1077488.033970	44.458561
3504.630398	1077408.319940	44.463565
3504.515959	1077309.079913	44.468570
3504.782763	1077233.006697	44.473575
3504.568085	1077146.643853	44.478580
3504.644709	1077050.631620	44.483585
3504.182294	1076967.762763	44.488589
3503.898309	1076890.911475	44.493594
3504.216105	1076807.239661	44.498599
3504.043665	1076737.664206	44.503604
3504.550873	1076658.087173	44.508609
3504.373583	1076578.525706	44.513613
3504.443697	1076500.554507	44.518618
3504.904692	1076418.389321	44.523623
3504.633320	1076329.622595	44.528628
3504.533491	1076245.530896	44.533633
3504.409097	1076165.954705	44.538637
3504.241000	1076081.295623	44.543642
3504.439744	1075991.581817	44.548647
3504.472944	1075920.809856	44.553652
3504.597472	1075837.251043	44.558657
3504.583318	1075755.154142	44.563661
3504.552514	1075671.138255	44.568666
3504.809937	1075585.729238	44.573671
3504.518213	1075514.717451	44.578676
3504.693658	1075422.693484	44.583681
3504.498810	1075323.622671	44.588685
3504.218932	1075249.052333	44.593690
3504.752470	1075174.058912	44.598695
3504.175847	1075099.727474	44.603700
3504.207349	1075013.866556	44.608705
3504.701950	1074924.278581	44.613709
3504.448695	1074851.235034	44.618714
3504.482442	1074772.764973	44.623719
3504.399214	1074687.398025	44.628724
3504.300887	1074601.359926	44.633729
3504.257507	1074526.260553	44.638733
3504.074371	1074457.522212	44.643738
3504.274659	1074370.374790	44.648743
3504.024168	1074300.012751	44.653748
3503.887486	1074217.144532	44.658753
3504.129684	1074145.642808	44.663757
3503.843199	1074067.023253	44.668762
3504.067541	1073992.160610	44.673767
3503.765657	1073915.942774	44.678772
3504.052188	1073843.661358	44.683777
3504.142116	1073783.418625	44.688781
3503.815671	1073702.879253	44.693786
3504.130013	1073629.341654	44.698791
3503.523133	1073566.521592	44.703796
3504.031348	1073492.277789	44.708801
3503.918479	1073418.135269	44.713805
3503.861187	1073350.707183	44.718810
3503.926839	1073277.205810	44.723815
3503.629345	1073217.885256	44.728820
3504.084122	1073138.265650	44.733825
3504.100835	1073080.044684	44.738829
3504.266713	1072996.627785	44.743834
3504.011868	1072927.305580	44.748839
3504.189958	1072852.531035	44.753844
3503.972914	1072776.955865	44.758849
3504.086430	1072700.268362	44.763853
3503.854261	1072637.471979	44.768858
3504.176246	1072566.416871	44.773863
3503.861415	1072495.753964	44.778868
3503.651446	1072417.962813	44.783873
3503.787508	1072344.725564	44.788877
3503.507255	1072285.776388	44.793882
3504.100163	1072223.511957	44.798887
3503.755940	1072154.867276	44.803892
3503.799478	1072076.933439	44.808897
3503.912939	1072001.965744	44.813901
3503.806587	1071946.731753	44.818906
3504.132398	1071874.129589	44.823911
3503.801956	1071805.862625	44.828916
3503.895500	1071737.524980	44.833921
3504.165417	1071670.791051	44.838925
3503.706440	1071600.716889	44.843930
3503.788705	1071526.900982	44.848935
3503.596583	1071461.970359	44.853940
3503.642449	1071398.825667	44.858945
3503.808393	1071334.603361	44.863949
3504.040811	1071262.873387	44.868954
3504.393176	1071182.088985	44.873959
3503.934091	1071116.429401	44.878964
3503.875536	1071049.934216	44.883969
3503.814250	1070979.402172	44.888973
3503.978327	1070909.504863	44.893978
3504.099132	1070824.716774	44.898983
3503.889914	1070765.739517	44.903988
3503.714978	1070695.703091	44.908993
3503.800359	1070617.164911	44.913997
3503.579347	1070560.686338	44.919002
3503.661472	1070491.662226	44.924007
3504.081708	1070418.256293	44.929012
3503.891401	1070357.445300	44.934017
3503.881356	1070279.590822	44.939021
3503.453321	1070223.142863	44.944026
3504.010038	1070137.215016	44.949031
3503.943855	1070086.857859	44.954036
3503.930526	1070016.593885	44.959041
3503.786057	1069938.660577	44.964045
3504.190464	1069869.287171	44.969050
3504.087496	1069793.555877	44.974055
3503.592286	1069729.327513	44.979060
3503.621532	1069671.741134	44.984065
3503.787947	1069609.421131	44.989069
3503.743512	1069540.502010	44.994074
3504.083334	1069463.347373	44.999079
3503.869973	1069400.510739	45.004084
3503.874400	1069321.005963	45.009089
3503.799139	1069261.509759	45.014093
3503.787431	1069192.388596	45.019098
3503.629107	1069125.309642	45.024103
3503.750535	1069064.432949	45.029108
3503.632189	1069003.498927	45.034113
3503.592151	1068928.899018	45.039117
3503.474605	1068864.790596	45.044122
3503.513430	1068801.520980	45.049127
3503.479572	1068746.338904	45.054132
3503.544877	1068693.639772	45.059137
3503.814054	1068624.753633	45.064141
3503.631811	1068558.921615	45.069146
3503.709773	1068489.007617	45.074151
3503.602113	1068434.123006	45.079156
3503.705285	1068370.164752	45.084161
3504.022351	1068303.285901	45.089165
3503.771069	1068241.980689	45.094170
3503.911026	1068161.859849	45.099175
3503.719607	1068098.812357	45.104180
3503.779908	1068023.606657	45.109185
3503.573849	1067963.444789	45.114189
3503.449912	1067901.826318	45.119194
3503.923187	1067842.897502	45.124199
3503.769803	1067785.994526	45.129204
3503.619948	1067716.877510	45.134209
3503.968333	1067649.312381	45.139213
3503.526478	1067589.281406	45.144218
3503.847396	1067516.237660	45.149223
3503.516311	1067453.205744	45.154228
3503.426726	1067382.055031	45.159233
3503.303035	1067319.083586	45.164237
3503.103027	1067265.452711	45.169242
3503.493703	1067217.205903	45.174247
3503.686559	1067145.236216	45.179252
3503.804978	1067072.893143	45.184257
3503.936490	1067006.221398	45.189261
3503.620179	1066962.993812	45.194266
3503.923096	1066889.752341	45.199271
3503.786761	1066826.969686	45.204276
3503.890173	1066759.049227	45.209281
3503.905432	1066685.371498	45.214285
3503.667968	1066629.624558	45.219290
3503.586618	1066550.574652	45.224295
3503.540305	1066495.949090	45.229300
3503.764089	1066427.812335	45.234305
3503.750970	1066354.615773	45.239309
3503.402727	1066295.998037	45.244314
3503.477191	1066232.692916	45.249319
3503.799631	1066167.807161	45.254324
3503.760064	1066094.130524	45.259329
3503.603226	1066034.612734	45.264333
3503.240510	1065976.667324	45.269338
3503.421300	1065931.810617	45.274343
3503.476668	1065870.620772	45.279348
3503.201191	1065809.677128	45.284353
3503.565499	1065760.171297	45.289357
3503.368017	1065708.929751	45.294362
3503.371336	1065637.644913	45.299367
3503.184840	1065571.392917	45.304372
3503.120693	1065514.355470	45.309377
3503.470832	1065459.173280	45.314381
3503.334215	1065405.321366	45.319386
3503.380520	1065347.398149	45.324391
3503.408171	1065287.649461	45.329396
3503.461219	1065238.478815	45.334401
3503.690778	1065158.972827	45.339405
3503.278290	1065107.761078	45.344410
3503.253081	1065041.764756	45.349415
3503.013291	1065000.337105	45.354420
3503.467117	1064933.587106	45.359425
3503.412726	1064879.427851	45.364429
3503.157003	1064824.531499	45.369434
3503.237940	1064766.788885	45.374439
3503.061367	1064711.012417	45.379444
3502.921724	1064643.105808	45.384449
3503.255623	1064602.061759	45.389453
3503.111761	1064551.666546	45.394458
3503.097069	1064492.301058	45.399463
3503.197333	1064444.847507	45.404468
3503.104482	1064392.710442	45.409473
3503.352738	1064324.447341	45.414477
3502.907785	1064286.127250	45.419482
3503.130959	1064231.338542	45.424487
3503.255503	1064186.669302	45.429492
3503.147264	1064131.356822	45.434497
3503.347129	1064063.483359	45.439501
3502.706801	1064024.231330	45.444506
3502.859155	1063979.940746	45.449511
3503.052085	1063921.593425	45.454516
3503.000526	1063888.979621	45.459521
3503.120571	1063820.057751	45.464525
3502.904106	1063770.437187	45.469530
3502.908403	1063711.733771	45.474535
3502.952772	1063670.153044	45.479540
3502.777030	1063621.294308	45.484545
3502.989388	1063569.484107	45.489549
3502.807766	1063526.592193	45.494554
3503.169991	1063473.697792	45.499559
3503.114146	1063429.918260	45.504564
3502.800202	1063370.686176	45.509569
3502.951981	1063309.933126	45.514573
3502.864841	1063286.753279	45.519578
3503.149783	1063238.777690	45.524583
3503.131165	1063177.185051	45.529588
3502.915227	1063121.206429	45.534593
3503.029175	1063072.968820	45.539597
3502.953445	1063033.809203	45.544602
3502.876382	1062995.034515	45.549607
3502.778350	1062937.013406	45.554612
3502.848311	1062890.995153	45.559617
3502.758818	1062849.141514	45.564621
3502.838255	1062797.923434	45.569626
3502.743078	1062747.022390	45.574631
3503.011719	1062696.927227	45.579636
3502.560088	1062650.415349	45.584641
3502.970337	1062606.841256	45.589645
3502.970107	1062554.671492	45.594650
3502.855657	1062500.594928	45.599655
3502.721978	1062455.376614	45.604660
3502.815394	1062413.393276	45.609665
3502.709148	1062359.313972	45.614669
3502.304436	1062321.839853	45.619674
3503.000311	1062270.322818	45.624679
3502.577564	1062238.915470	45.629684
3502.524914	1062194.548007	45.634689
3502.770761	1062151.189908	45.639693
3502.758031	1062114.034861	45.644698
3502.871716	1062068.483837	45.649703
3502.585419	1062026.560083	45.654708
3502.609452	1061986.028872	45.659713
3502.537697	1061932.998605	45.664717
3503.088146	1061898.733590	45.669722
3502.904289	1061850.726840	45.674727
3503.068288	1061801.218361	45.679732
3502.467718	1061746.540564	45.684737
3502.825297	1061704.604580	45.689741
3502.704192	1061663.228466	45.694746
3502.666358	1061607.205085	45.699751
3502.549157	1061579.209411	45.704756
3502.359481	1061519.744356	45.709761
3502.890868	1061488.849486	45.714765
3502.595079	1061440.376219	45.719770
3502.611133	1061391.658616	45.724775
3502.383596	1061347.698224	45.729780
3502.603769	1061306.937154	45.734785
3502.553103	1061265.450169	45.739789
3502.384440	1061233.995223	45.744794
3502.676180	1061195.339656	45.749799
3502.619192	1061152.312400	45.754804
3502.536810	1061105.245222	45.759809
3502.500763	1061060.577035	45.764813
3502.531588	1061012.046199	45.769818
3502.606246	1060905.930353	45.774823
3502.703331	1060742.614838	45.779828
3502.341146	1060516.107594	45.784833
3502.499629	1060238.180061	45.789837
3502.476072	1059890.065136	45.794842
3502.344328	1059481.849756	45.799847
3502.575927	1059011.709191	45.804852
3502.499215	1058491.008377	45.809857
3502.688216	1057884.283028	45.814861
3502.177397	1057209.295562	45.819866
3502.089423	1056474.123058	45.824871
3501.893546	1055679.407173	45.829876
3501.789432	1054815.643096	45.834881
3501.924057	1053865.517481	45.839885
3501.434744	1052869.529799	45.844890
3501.355805	1051780.903085	45.849895
3500.997038	1050632.590481	45.854900
3500.822289	1049395.147236	45.859905
3500.801136	1048084.249531	45.864909
3500.374867	1046702.061152	45.869914
3500.322799	1045239.517352	45.874919
3499.952989	1043692.998664	45.879924
3499.782545	1042075.296094	45.884929
3499.368193	1040367.382449	45.889933
3499.403236	1038608.406727	45.894938
3499.105915	1036753.288903	45.899943
3498.814947	1034806.811333	45.904948
3498.290549	1032785.660399	45.909953
3498.060801	1030665.369370	45.914957
3497.665482	1028490.549333	45.919962
3497.497816	1026219.992753	45.924967
3496.995316	1023880.623031	45.929972
3496.749406	1021445.494099	45.934977
3496.615265	1018931.289991	45.939981
3496.179574	1016343.312449	45.944986
3495.911396	1013650.990323	45.949991
3494.951240	1010882.686111	45.954996
3494.833275	1008044.258136	45.960001
3494.536194	1005110.388671	45.965005
3493.801243	1002107.927459	45.970010
3493.783755	999002.600226	45.975015
3493.474208	995825.189614	45.980020
3492.467701	992570.283833	45.985025
3492.167633	989212.848199	45.990029
3491.512992	985787.522537	45.995034
3491.054078	982278.865567	46.000039
3490.679278	978700.034560	46.005044
3489.908210	975023.020221	46.010049
3489.662662	971258.933071	46.015053
3488.672436	967425.046696	46.020058
3488.031129	963519.283669	46.025063
3487.505809	959512.721129	46.030068
3486.855836	955431.290403	46.035073
3486.470460	951344.584472	46.040077
3485.653335	947199.487891	46.045082
3484.424747	942980.014844	46.050087
3483.885045	938674.322422	46.055092
3483.172087	934293.891321	46.060097
3482.569463	929838.233531	46.065101
3481.712398	925291.292465	46.070106
3481.265710	920652.185607	46.075111
3480.111149	915944.017064	46.080116
3479.227035	911170.054256	46.085121
3478.270863	906284.776412	46.090125
3477.123154	901336.533409	46.095130
3476.447907	896300.736074	46.100135
3475.844395	891197.873394	46.105140
3474.505583	886005.579543	46.110145
3473.348867	880721.866696	46.115149
3472.585264	875386.476160	46.120154
3471.489733	869937.493285	46.125159
3470.365709	864429.236882	46.130164
3469.166563	858835.639737	46.135169
3468.277878	853157.732634	46.140173
3467.321882	847414.999989	46.145178
3466.230681	841576.028877	46.150183
3465.237673	835654.790818	46.155188
3463.827970	829653.462930	46.160193
3463.107560	823552.200753	46.165197
3461.455000	817401.397255	46.170202
3460.510186	811156.330353	46.175207
3459.178458	804827.301166	46.180212
3457.949804	798423.997541	46.185217
3456.989270	791927.307927	46.190221
3455.572813	785366.348663	46.195226
3454.248139	778710.670900	46.200231
3453.364295	771974.636985	46.205236
3451.563585	765155.488834	46.210241
3450.444894	758250.517201	46.215245
3449.236243	751287.091817	46.220250
3447.657074	744214.767831	46.225255
3446.548721	737073.116590	46.230260
3444.956542	729853.851096	46.235265
3443.412808	722532.745044	46.240269
3441.901790	715148.658124	46.245274
3440.591875	707685.178356	46.250279
3439.152048	700134.722591	46.255284
3437.265558	692517.796402	46.260289
3435.861250	684810.653531	46.265293
3434.211478	677046.364639	46.270298
3432.418807	669191.685931	46.275303
3431.088810	661247.233106	46.280308
3429.546151	653232.877704	46.285313
3427.833546	645144.991031	46.290317
3426.201387	636983.907441	46.295322
3424.518492	628753.486642	46.300327
3423.132715	620424.847900	46.305332
3420.890295	612028.062672	46.310337
3419.188950	603559.749304	46.315341
3417.390347	595028.009835	46.320346
3415.284566	586415.719819	46.325351
3413.546582	577730.970144	46.330356
3411.520817	568980.389098	46.335361
3409.831755	560143.720375	46.340365
3407.685336	551252.460158	46.345370
3405.510861	542279.533216	46.350375
3403.711566	533234.649582	46.355380
3401.366971	524141.606590	46.360385
3399.410419	514961.351270	46.365389
3397.266494	505731.694398	46.370394
3395.123448	496414.430361	46.375399
3393.026601	487054.765064	46.380404
3390.830751	477618.886060	46.385409
3388.770782	468119.570196	46.390413
3386.045468	458546.834955	46.395418
3383.972520	448922.794740	46.400423
3381.945634	439239.283568	46.405428
3378.776933	429487.512747	46.410433
3376.315601	419680.960134	46.415437
3374.065697	409796.335307	46.420442
3371.419796	399866.236822	46.425447
3369.058384	389898.043734	46.430452
3366.129909	379867.775172	46.435457
3363.553404	369782.289007	46.440461
3360.591237	359660.636432	46.445466
3357.984260	349478.854170	46.450471
3355.393270	339256.557520	46.455476
3351.752315	329003.195751	46.460481
3349.078254	318676.704536	46.465485
3345.961612	308327.455227	46.470490
3342.784693	297937.618964	46.475495
3339.334422	287513.884281	46.480500
3335.962456	277049.891386	46.485505
3332.794221	266560.588156	46.490509
3329.357868	256039.965148	46.495514
3325.741268	245480.906635	46.500519
3322.252689	234921.317010	46.505524
3318.540864	224252.122297	46.510529
3314.748493	213631.559904	46.515533
3311.194229	203008.047785	46.520538
3307.021731	192357.102701	46.525543
3302.909291	181717.274504	46.530548
3298.544611	171062.990160	46.535553
3293.938567	160411.877861	46.540557
3289.402244	149772.446936	46.545562
3284.830714	139140.808149	46.550567
3279.790839	128511.783466	46.555572
3274.611485	117919.022269	46.560577
3269.178322	107348.706631	46.565581
3263.546861	96803.737099	46.570586
3256.970287	86310.793460	46.575591
3250.985357	75873.986088	46.580596
3243.761158	65517.617235	46.585601
3236.994165	55214.354800	46.590605
3228.068248	45058.432435	46.595610
3214.318286	35131.894926	46.600615
3180.110340	25917.378569	46.605620
3125.733500	17652.499833	46.610625
3067.503208	10196.549002	46.615629
3010.332454	3691.875401	46.620634
2876.291239	434.070924	46.625639
2692.693223	386.857465	46.630644
2611.548689	378.769810	46.635649
2623.203603	378.991769	46.640653
2688.494032	372.363359	46.645658
2766.460977	369.659915	46.650663
2828.372318	357.000344	46.655668
2862.841580	341.374894	46.660673
2873.452030	342.242271	46.665677
2868.076272	340.681129	46.670682
2856.342526	349.625800	46.675687
2845.079835	345.906684	46.680692
2836.289987	357.773443	46.685697
2831.750248	338.284028	46.690701
2829.810879	326.624047	46.695706
2827.832039	335.499883	46.700711
2826.768687	338.606801	46.705716
2824.762241	338.203246	46.710721
2823.307493	331.733897	46.715725
2820.433570	330.734403	46.720730
2817.026685	326.373383	46.725735
2814.194868	321.151678	46.730740
2810.602030	334.514094	46.735745
2807.516608	327.068808	46.740749
2804.906685	317.259128	46.745754
2801.894308	304.982264	46.750759
2799.223996	312.422366	46.755764
2795.469530	320.892722	46.760769
2792.333457	312.786996	46.765773
2789.064943	317.089637	46.770778
2785.840779	329.775453	46.775783
2782.778669	305.306331	46.780788
2779.937451	312.820391	46.785793
2776.580506	306.287690	46.790797
2773.188470	305.768067	46.795802
2769.712148	317.619662	46.800807
2766.118556	306.107439	46.805812
2762.995763	311.236693	46.810817
2759.859965	305.302900	46.815821
2756.827520	302.264259	46.820826
2753.177299	310.201557	46.825831
2750.062201	301.555306	46.830836
2746.316067	314.112298	46.835841
2742.970489	300.986002	46.840845
2740.057261	295.296605	46.845850
2736.725224	312.624207	46.850855
2733.543930	296.741756	46.855860
2729.641920	306.392727	46.860865
2726.380414	304.611670	46.865869
2723.172768	303.273490	46.870874
2719.424204	292.064578	46.875879
2715.997381	297.580195	46.880884
2712.299087	295.299732	46.885889
2709.250218	295.724938	46.890893
2705.767241	295.066729	46.895898
2702.494665	300.937051	46.900903
2699.515519	289.270991	46.905908
2695.703539	285.757609	46.910913
2692.345440	286.940294	46.915917
2688.824914	295.767529	46.920922
2684.947189	293.204904	46.925927
2682.018756	291.443441	46.930932
2678.965950	289.476855	46.935937
2675.444759	281.834461	46.940941
2672.045281	284.915246	46.945946
2667.851634	289.853879	46.950951
2664.772968	287.660111	46.955956
2661.700616	283.923578	46.960961
2658.271183	287.979904	46.965965
2654.699824	280.347569	46.970970
2651.090916	285.741691	46.975975
2647.490330	272.787748	46.980980
2644.368611	278.565629	46.985985
2640.890084	283.823124	46.990989
2637.360122	269.119491	46.995994
2633.937105	280.338303	47.000999
2630.247985	274.671129	47.006004
2626.669711	280.418730	47.011009
2623.216379	280.433647	47.016013
2619.389772	275.270203	47.021018
2616.383546	268.480977	47.026023
2613.363597	260.493849	47.031028
2609.028015	277.728624	47.036033
2605.551522	269.522672	47.041037
2602.465873	267.913645	47.046042
2598.784192	269.577007	47.051047
2595.607945	268.023174	47.056052
2592.270306	268.359891	47.061057
2589.161759	277.360935	47.066061
2586.186272	271.997880	47.071066
2582.510809	270.554384	47.076071
2578.817152	259.483429	47.081076
2574.600589	271.265317	47.086081
2571.112481	261.257546	47.091085
2567.923589	256.289300	47.096090
2564.478137	268.923121	47.101095
2560.999650	260.188328	47.106100
2557.339345	258.812886	47.111105
2554.220423	261.692267	47.116109
2550.257748	247.256289	47.121114
2547.121933	256.286495	47.126119
2543.823753	255.201781	47.131124
2540.151522	253.504915	47.136129
2536.940704	249.953767	47.141133
2533.094254	250.971385	47.146138
2529.769658	263.607582	47.151143
2526.526204	246.860757	47.156148
2523.049805	250.849598	47.161153
2519.470369	254.108297	47.166157
2515.833951	253.094760	47.171162
2512.018890	251.540737	47.176167
2508.845568	246.694658	47.181172
2505.282072	258.712996	47.186177
2501.703791	256.108103	47.191181
2498.605545	254.979095	47.196186
2494.537544	263.527484	47.201191
2491.488289	247.679392	47.206196
2487.743294	252.396726	47.211201
2484.749590	245.997473	47.216205
2481.087061	252.727832	47.221210
2477.083400	244.353864	47.226215
2473.711605	254.124655	47.231220
2470.678175	253.952997	47.236225
2467.415155	240.100993	47.241229
2463.781965	254.589966	47.246234
2460.173925	251.986253	47.251239
2456.498912	241.072432	47.256244
2452.928202	248.163544	47.261249
2449.175193	242.351335	47.266253
2445.832192	235.177136	47.271258
2442.147064	243.981162	47.276263
2439.271212	236.111843	47.281268
2435.974803	236.802126	47.286273
2432.213975	242.211510	47.291277
2428.997514	241.388626	47.296282
2425.241136	246.909158	47.301287
2421.926259	238.275531	47.306292
2418.485372	238.109624	47.311297
2414.736081	229.318759	47.316301
2411.312227	244.944576	47.321306
2407.550792	249.908340	47.326311
2404.410549	242.477855	47.331316
2400.935082	244.635610	47.336321
2396.964969	245.681581	47.341325
2393.531877	237.554042	47.346330
2389.971984	237.829927	47.351335
2386.953393	239.240192	47.356340
2383.179239	247.035257	47.361345
2380.094796	232.952994	47.366349
2376.769407	239.341489	47.371354
2372.740756	237.265746	47.376359
2369.423144	229.879037	47.381364
2365.177838	244.051561	47.386369
2362.303789	241.138517	47.391373
2358.999521	240.055877	47.396378
2355.555846	219.445642	47.401383
2351.956137	238.530581	47.406388
2347.948649	240.747289	47.411393
2344.772060	228.010837	47.416397
2341.296255	225.945161	47.421402
2337.912272	234.112056	47.426407
2334.863652	223.486194	47.431412
2331.064750	233.669206	47.436417
2327.597162	240.186438	47.441421
2323.945319	238.406310	47.446426
2320.043970	235.379659	47.451431
2316.599415	224.796806	47.456436
2313.398731	233.176472	47.461441
2309.974322	228.207538	47.466445
2306.823432	223.419819	47.471450
2303.068906	227.463986	47.476455
2299.188574	225.476589	47.481460
2295.328512	226.580625	47.486465
2292.162262	226.247344	47.491469
2288.756633	220.372615	47.496474
2285.670017	230.064655	47.501479
2282.260975	228.809514	47.506484
2278.311812	231.529950	47.511489
2275.231525	224.445211	47.516493
2271.244195	222.798084	47.521498
2268.084700	223.773964	47.526503
2265.253328	219.728645	47.531508
2261.198424	223.075439	47.536513
2257.427272	222.684284	47.541517
2254.011645	216.800371	47.546522
2250.037783	232.263484	47.551527
2247.169453	230.957361	47.556532
2243.309089	232.437750	47.561537
2240.079203	234.415570	47.566541
2236.622714	225.519793	47.571546
2232.706829	219.661966	47.576551
2229.628896	222.446898	47.581556
2225.708082	229.459195	47.586561
2222.313519	214.227926	47.591565
2219.153484	228.196145	47.596570
2215.392184	227.510868	47.601575
2212.319881	217.987426	47.606580
2208.382753	223.557688	47.611585
2205.152940	226.011430	47.616589
2201.851230	215.522689	47.621594
2197.777409	223.950702	47.626599
2194.654085	221.926605	47.631604
2190.987429	219.801027	47.636609
2187.596159	222.060908	47.641613
2184.062333	222.485904	47.646618
2180.437166	226.270830	47.651623
2177.331356	212.874437	47.656628
2173.269374	216.552745	47.661633
2169.927092	217.979091	47.666637
2166.748213	216.763587	47.671642
2162.902995	221.997187	47.676647
2159.682432	222.949936	47.681652
2155.961940	222.118261	47.686657
2152.415246	218.671632	47.691661
2149.052246	211.600640	47.696666
2145.176465	228.013361	47.701671
2142.038312	214.229962	47.706676
2138.687599	216.697062	47.711681
2135.226293	221.093290	47.716685
2131.859462	212.409701	47.721690
2128.143883	218.966625	47.726695
2124.348733	213.327305	47.731700
2120.736243	213.814140	47.736705
2117.739445	217.348447	47.741709
2114.127948	212.762487	47.746714
2110.544927	222.933254	47.751719
2106.961244	209.377175	47.756724
2103.857685	202.838092	47.761729
2099.996946	210.574239	47.766733
2096.382425	194.873931	47.771738
2092.810950	202.219729	47.776743
2089.875526	204.960981	47.781748
2086.143611	201.300965	47.786753
2082.223034	202.433932	47.791757
2078.947888	203.964770	47.796762
2075.480135	208.646115	47.801767
2072.189291	200.942321	47.806772
2068.519932	206.877208	47.811777
2064.871738	209.764259	47.816781
2061.866633	202.336733	47.821786
2057.970565	219.107098	47.826791
2054.666487	210.939239	47.831796
2051.004028	209.771591	47.836801
2047.603958	206.814538	47.841805
2044.293469	209.407932	47.846810
2040.405047	212.763680	47.851815
2037.262401	204.786151	47.856820
2033.554546	198.410618	47.861825
2029.808066	200.054743	47.866829
2026.578115	198.135822	47.871834
2022.885520	198.150233	47.876839
2019.892613	201.769170	47.881844
2016.225900	193.208624	47.886849
2012.287340	196.655525	47.891853
2009.102628	200.345174	47.896858
2005.694756	195.495028	47.901863
2002.464966	197.161074	47.906868
1998.553675	199.465974	47.911873
1994.635927	202.543534	47.916877
1991.565625	204.152889	47.921882
1987.563771	210.277920	47.926887
1984.619234	203.148643	47.931892
1981.033616	201.015432	47.936897
1977.769928	194.713955	47.941901
1974.076054	203.914215	47.946906
1970.448361	196.610258	47.951911
1967.036914	194.414977	47.956916
1963.822899	208.114633	47.961921
1960.006533	194.801955	47.966925
1956.683771	200.369535	47.971930
1953.011747	203.771708	47.976935
1949.776442	198.531545	47.981940
1946.361826	204.826288	47.986945
1942.346495	206.217261	47.991949
1938.975091	194.401508	47.996954
1935.550081	188.540731	48.001959
1932.186513	200.152629	48.006964
1928.625288	200.538758	48.011969
1925.007934	208.818481	48.016973
1921.519541	198.980466	48.021978
1918.110680	213.059258	48.026983
1914.292260	191.159099	48.031988
1910.701970	193.257972	48.036993
1907.612455	201.157609	48.041997
1903.888055	192.953128	48.047002
1900.296238	197.087244	48.052007
1897.137685	196.574889	48.057012
1893.680056	197.801959	48.062017
1890.239792	194.066411	48.067021
1887.063358	186.609530	48.072026
1883.006319	204.084167	48.077031
1879.499685	193.578819	48.082036
1875.824111	185.086712	48.087041
1872.508187	189.205412	48.092045
1869.284873	199.701771	48.097050
1865.458113	202.392549	48.102055
1862.109301	188.363906	48.107060
1858.430362	205.750425	48.112065
1854.687764	194.918696	48.117069
1851.249732	184.236409	48.122074
1848.064369	185.106827	48.127079
1844.909128	188.482587	48.132084
1841.017795	184.245826	48.137089
1837.589524	189.168874	48.142093
1834.130368	190.523292	48.147098
1830.529908	196.236380	48.152103
1827.341449	185.499218	48.157108
1823.638218	199.732453	48.162113
1819.827683	205.277370	48.167117
1816.757233	202.520781	48.172122
1812.838723	198.912814	48.177127
1809.073374	197.750329	48.182132
1806.089136	198.605439	48.187137
1802.381406	188.653534	48.192141
1798.882533	185.915847	48.197146
1795.745989	193.963666	48.202151
1791.898221	197.435161	48.207156
1788.172726	192.314039	48.212161
1784.679001	194.348796	48.217165
1781.841062	196.243095	48.222170
1778.305899	192.419477	48.227175
1774.552182	190.306809	48.232180
1771.076919	188.670289	48.237185
1767.621636	188.733281	48.242189
1764.075862	182.630393	48.247194
1760.290341	187.929103	48.252199
1756.760538	185.665750	48.257204
1753.322288	185.804765	48.262209
1749.941296	194.703887	48.267213
1746.649958	194.948102	48.272218
1742.933846	198.424634	48.277223
1739.419412	182.694054	48.282228
1735.895391	190.799116	48.287233
1732.315106	198.096001	48.292237
1729.272802	186.763360	48.297242
1725.005764	179.974862	48.302247
1721.820527	185.622738	48.307252
1718.694250	188.069262	48.312257
1715.265499	184.728802	48.317261
1711.651036	180.857140	48.322266
1708.017233	198.939967	48.327271
1704.531340	179.875351	48.332276
1700.722419	188.932901	48.337281
1697.553324	195.101201	48.342285
1694.107380	190.847663	48.347290
1690.345938	187.483580	48.352295
1686.873608	183.355551	48.357300
1683.215242	187.301458	48.362305
1679.411661	189.604040	48.367309
1676.246565	184.894650	48.372314
1672.853850	190.105008	48.377319
1669.730759	181.114414	48.382324
1666.064505	192.539568	48.387329
1662.461909	188.841186	48.392333
1658.978459	189.411630	48.397338
1655.405057	185.426969	48.402343
1652.115992	185.852479	48.407348
1648.313997	184.996636	48.412353
1644.717543	192.895658	48.417357
1641.583609	186.363995	48.422362
1637.823898	193.520244	48.427367
1634.457711	187.975290	48.432372
1630.489347	184.357014	48.437377
1626.828074	186.842134	48.442381
1623.788221	181.970138	48.447386
1620.066952	191.254869	48.452391
1617.251491	193.020721	48.457396
1613.748597	182.831017	48.462401
1610.049582	186.459483	48.467405
1606.555677	187.504831	48.472410
1602.979841	188.720663	48.477415
1599.633593	178.542414	48.482420
1595.725465	182.771185	48.487425
1591.726383	199.809281	48.492429
1588.825904	189.631955	48.497434
1585.169870	192.724644	48.502439
1582.282313	192.385345	48.507444
1578.264633	179.570730	48.512449
1574.671821	186.176882	48.517453
1571.566998	190.871257	48.522458
1567.471609	185.157315	48.527463
1564.177307	180.270808	48.532468
1560.843289	184.156144	48.537473
1557.077013	184.420911	48.542477
1553.984499	180.294698	48.547482
1550.644532	190.008927	48.552487
1547.315965	178.429736	48.557492
1543.551453	176.727512	48.562497
1539.694781	175.393885	48.567501
1536.175520	176.177672	48.572506
1532.585781	188.012200	48.577511
1529.397696	173.775923	48.582516
1526.068776	171.707338	48.587521
1522.121436	182.323779	48.592525
1518.895987	177.527056	48.597530
1515.276790	179.845167	48.602535
1511.769632	181.228178	48.607540
1508.368715	182.510294	48.612545
1504.850004	179.227311	48.617549
1501.409581	174.735800	48.622554
1497.819867	187.408714	48.627559
1494.292402	163.797759	48.632564
1490.797431	182.278097	48.637569
1487.038814	185.550938	48.642573
1484.000955	166.120630	48.647578
1479.958293	183.689805	48.652583
1476.668370	180.316594	48.657588
1473.055344	184.835806	48.662593
1469.618722	179.891839	48.667597
1466.417338	178.656298	48.672602
1462.642025	179.778742	48.677607
1459.143408	169.035963	48.682612
1455.786682	176.672432	48.687617
1452.317818	173.480796	48.692621
1448.997175	173.628369	48.697626
1445.190335	179.142756	48.702631
1441.909693	184.604931	48.707636
1438.372401	180.963082	48.712641
1434.821302	172.354615	48.717645
1431.204374	176.675007	48.722650
1427.345230	188.625563	48.727655
1424.432841	171.323896	48.732660
1420.572418	171.409034	48.737665
1417.179959	177.294851	48.742669
1413.891489	170.204183	48.747674
1409.955876	174.882421	48.752679
1406.415217	174.186120	48.757684
1403.287518	168.921581	48.762689
1399.627038	172.376762	48.767693
1396.393580	168.595311	48.772698
1392.701394	179.248029	48.777703
1389.206553	171.725384	48.782708
1385.609494	166.213744	48.787713
1382.102362	179.414882	48.792717
1378.883066	171.811743	48.797722
1374.903994	169.529810	48.802727
1371.649341	179.638945	48.807732
1368.216152	176.883541	48.812737
1364.590989	169.110526	48.817741
1361.408141	172.213024	48.822746
1357.470604	174.606938	48.827751
1354.282941	163.726186	48.832756
1351.000936	161.747912	48.837761
1347.367619	171.405159	48.842765
1343.755600	169.808104	48.847770
1339.935917	168.330367	48.852775
1336.890419	174.742498	48.857780
1333.163409	172.701535	48.862785
1329.681093	163.977505	48.867789
1326.280255	161.661329	48.872794
1322.568590	174.196775	48.877799
1318.894441	168.985280	48.882804
1315.646502	165.899613	48.887809
1312.108002	172.104657	48.892813
1308.463509	165.209254	48.897818
1304.738220	174.216467	48.902823
1301.575421	168.955603	48.907828
1298.154041	160.879865	48.912833
1294.557468	164.754191	48.917837
1291.401773	155.362837	48.922842
1287.448431	173.350727	48.927847
1284.360407	161.871699	48.932852
1280.723663	161.401460	48.937857
1276.951460	170.935849	48.942861
1273.663205	159.706034	48.947866
1270.162541	166.276089	48.952871
1266.747888	165.983281	48.957876
1263.195752	164.028229	48.962881
1259.239382	168.136485	48.967885
1256.026040	159.431046	48.972890
1252.372076	164.987472	48.977895
1249.083737	159.397528	48.982900
1245.490561	166.534645	48.987905
1242.055284	169.620555	48.992909
1238.405825	161.053114	48.997914
1234.998924	168.444801	49.002919
1231.722365	166.179387	49.007924
1228.375778	164.248730	49.012929
1224.569064	156.169656	49.017933
1221.067238	163.371516	49.022938
1217.382345	168.649727	49.027943
1214.113312	164.966386	49.032948
1210.555835	157.871802	49.037953
1206.835864	170.099673	49.042957
1203.438783	160.863539	49.047962
1199.843926	166.136168	49.052967
1196.284612	160.483350	49.057972
1193.348048	174.382669	49.062977
1189.752425	177.338112	49.067981
1186.561978	162.067845	49.072986
1182.328778	154.383285	49.077991
1178.634476	165.787200	49.082996
1175.597022	163.662489	49.088001
1171.747485	164.707563	49.093005
1168.512343	166.141435	49.098010
1164.863681	165.075570	49.103015
1161.382856	151.396630	49.108020
1158.227368	157.717076	49.113025
1154.540054	161.859599	49.118029
1151.503768	151.021760	49.123034
1147.294716	163.687916	49.128039
1143.819782	151.821795	49.133044
1140.498093	156.575118	49.138049
1136.722698	158.267088	49.143053
1133.451078	158.805188	49.148058
1129.854268	156.532121	49.153063
1126.467956	165.218362	49.158068
1122.994032	158.872247	49.163073
1119.579962	166.770181	49.168077
1116.245059	156.023880	49.173082
1112.414408	169.728286	49.178087
1108.770164	158.956894	49.183092
1105.810677	158.352449	49.188097
1102.212447	160.762406	49.193101
1098.548803	153.637569	49.198106
1094.541987	155.461685	49.203111
1091.416753	151.593963	49.208116
1087.937438	142.304597	49.213121
1083.975253	150.547260	49.218125
1080.883252	146.317320	49.223130
1077.377444	154.316636	49.228135
1074.000478	146.406252	49.233140
1070.412610	158.217248	49.238145
1066.743915	169.951032	49.243149
1063.653415	158.188612	49.248154
1059.804625	156.286099	49.253159
1056.464596	164.413836	49.258164
1053.233999	156.654506	49.263169
1049.477132	166.283736	49.268173
1046.103533	163.242629	49.273178
1042.518096	164.661287	49.278183
1038.530882	149.467225	49.283188
1035.464420	156.468343	49.288193
1031.486552	169.250885	49.293197
1028.199531	159.459704	49.298202
1024.958733	146.708151	49.303207
1021.303263	153.005930	49.308212
1017.855438	155.092172	49.313217
1014.698106	161.294100	49.318221
1011.063949	155.878978	49.323226
1006.982260	166.068153	49.328231
1003.910629	154.709214	49.333236
1000.541840	157.187395	49.338241
996.819108	162.444629	49.343245
993.684218	159.166533	49.348250
989.864491	165.688860	49.353255
986.154222	155.938582	49.358260
982.661822	152.556048	49.363265
978.865077	163.925362	49.368269
975.748052	157.051796	49.373274
972.272194	151.824940	49.378279
969.093776	141.925211	49.383284
965.759639	155.437392	49.388289
961.287037	164.756078	49.393293
958.304847	148.491866	49.398298
954.665772	155.172909	49.403303
951.459555	159.419795	49.408308
948.059561	163.505215	49.413313
944.100908	153.668415	49.418317
941.163333	158.332064	49.423322
937.409480	159.343415	49.428327
933.781468	161.243788	49.433332
929.873016	157.480306	49.438337
926.375643	161.624137	49.443341
923.155757	152.156774	49.448346
919.650647	145.562488	49.453351
916.365235	154.558401	49.458356
913.095361	156.016080	49.463361
909.155756	156.914968	49.468365
905.722175	160.325232	49.473370
902.366806	159.918343	49.478375
898.854474	155.328252	49.483380
895.545830	157.121158	49.488385
891.782499	160.620109	49.493389
888.560058	157.746407	49.498394
884.797376	148.434498	49.503399
881.180101	161.571320	49.508404
877.911549	151.404860	49.513409
873.857652	157.141349	49.518413
870.686597	153.068701	49.523418
867.083043	153.162839	49.528423
863.561286	148.491951	49.533428
860.667073	156.157251	49.538433
856.567634	162.248240	49.543437
853.154729	150.578648	49.548442
849.759552	150.225418	49.553447
845.780924	147.161796	49.558452
842.628495	151.778977	49.563457
838.943661	162.152793	49.568461
836.006920	143.456117	49.573466
832.141813	158.260306	49.578471
828.366334	160.765768	49.583476
825.206307	151.180946	49.588481
821.462055	151.574378	49.593485
818.430722	151.672215	49.598490
814.835167	151.542692	49.603495
811.239327	159.186148	49.608500
807.721967	151.389666	49.613505
804.200854	150.431092	49.618509
800.722359	149.573706	49.623514
796.879386	154.497610	49.628519
793.417656	147.731283	49.633524
790.544428	142.366546	49.638529
786.427168	161.224888	49.643533
783.253410	139.379157	49.648538
779.706467	139.755815	49.653543
776.048489	149.166192	49.658548
772.728837	154.022927	49.663553
769.085580	152.429868	49.668557
765.522370	151.870222	49.673562
762.146761	160.235791	49.678567
758.719677	143.440422	49.683572
755.211500	148.454378	49.688577
751.405698	150.105702	49.693581
748.228568	143.804128	49.698586
744.379445	156.570561	49.703591
741.366962	144.248318	49.708596
737.734468	152.700217	49.713601
733.873261	147.997657	49.718605
730.904087	150.122886	49.723610
727.232575	147.540569	49.728615
723.622573	156.391669	49.733620
720.251546	148.436709	49.738625
716.222900	148.214205	49.743629
712.918786	137.340255	49.748634
709.331741	146.689421	49.753639
705.917870	154.622217	49.758644
702.809264	137.406218	49.763649
699.328858	141.362274	49.768653
695.600582	137.500526	49.773658
691.797709	131.054113	49.778663
688.614997	139.341380	49.783668
685.107508	142.383834	49.788673
681.637268	135.641084	49.793677
678.041446	134.539142	49.798682
674.758703	146.143728	49.803687
671.033130	140.584191	49.808692
667.949727	134.753949	49.813697
663.822337	148.424762	49.818701
660.335697	140.689797	49.823706
656.937824	146.370442	49.828711
653.438000	139.883472	49.833716
650.296023	129.230511	49.838721
646.412751	147.240296	49.843725
642.869338	138.111946	49.848730
639.449605	136.829410	49.853735
635.982726	140.487298	49.858740
632.682837	135.458093	49.863745
628.919216	132.264197	49.868749
625.943833	137.665633	49.873754
622.407069	135.138470	49.878759
618.460234	139.040883	49.883764
614.939921	132.034157	49.888769
610.801167	141.871470	49.893773
607.904307	138.986368	49.898778
604.444170	134.660713	49.903783
600.720293	135.542205	49.908788
597.443249	139.423288	49.913793
593.975557	135.788581	49.918797
590.870397	129.370245	49.923802
586.839782	141.777125	49.928807
583.333846	147.643168	49.933812
579.732415	135.322802	49.938817
575.904295	148.171565	49.943821
572.964977	128.367809	49.948826
569.611347	135.670661	49.953831
566.271760	137.513820	49.958836
562.439473	130.336978	49.963841
559.102766	142.461253	49.968845
556.006329	151.034041	49.973850
551.750200	144.513212	49.978855
548.058488	139.420815	49.983860
545.080674	136.959616	49.988865
541.245649	146.185852	49.993869
537.685111	139.141321	49.998874
534.182162	127.382744	50.003879
530.535103	138.430962	50.008884
527.709802	140.760208	50.013889
524.271955	138.269641	50.018893
520.693804	133.102667	50.023898
516.828473	142.877110	50.028903
513.609056	134.952683	50.033908
510.169804	146.237496	50.038913
506.064735	142.954259	50.043917
502.783805	138.260972	50.048922
499.487015	141.818420	50.053927
495.871246	138.303824	50.058932
492.351374	132.621242	50.063937
488.728650	145.802222	50.068941
485.716348	135.568822	50.073946
481.542728	141.313755	50.078951
477.921117	142.087167	50.083956
475.077549	143.248423	50.088961
471.653783	150.177564	50.093965
467.953108	132.869909	50.098970
464.001116	142.027994	50.103975
460.744082	147.537977	50.108980
457.635069	127.479980	50.113985
453.718681	140.593856	50.118989
450.494106	145.625334	50.123994
446.791343	141.304034	50.128999
443.402484	140.589488	50.134004
439.766342	137.496289	50.139009
435.934967	147.432582	50.144013
432.751282	132.361193	50.149018
429.544196	141.455735	50.154023
426.062644	143.380621	50.159028
422.531058	139.645185	50.164033
418.698733	143.743466	50.169037
415.336277	133.984863	50.174042
411.422078	138.016269	50.179047
408.252561	137.098487	50.184052
404.785639	134.011787	50.189057
401.037313	153.894833	50.194061
397.487668	148.488520	50.199066
394.038430	147.938861	50.204071
390.536277	142.900188	50.209076
387.315693	140.619554	50.214081
383.648005	144.167888	50.219085
380.507103	142.484865	50.224090
376.786678	148.446026	50.229095
373.125965	140.321699	50.234100
369.670138	133.988245	50.239105
366.137584	145.801237	50.244109
362.823316	138.759047	50.249114
359.397668	136.196413	50.254119
355.549559	137.010960	50.259124
352.469815	138.919524	50.264129
348.829615	137.182364	50.269133
345.831426	140.017930	50.274138
341.933269	144.230914	50.279143
337.981235	134.896797	50.284148
334.523775	133.706092	50.289153
330.814966	139.585840	50.294157
327.781293	122.975105	50.299162
324.212737	136.971948	50.304167
320.486578	136.319110	50.309172
317.247398	130.237672	50.314177
313.786581	143.734110	50.319181
310.503938	129.380288	50.324186
306.620064	135.745639	50.329191
303.194419	135.990641	50.334196
300.069912	135.068634	50.339201
296.339072	135.571135	50.344205
292.853063	132.620342	50.349210
289.118053	140.798646	50.354215
285.460761	144.885645	50.359220
282.220857	141.061752	50.364225
278.177582	150.666730	50.369229
275.133050	147.755178	50.374234
271.569092	142.021408	50.379239
267.986838	148.747750	50.384244
264.791328	129.878557	50.389249
260.993848	145.564825	50.394253
257.202723	141.661835	50.399258
254.103678	143.133734	50.404263
250.654061	132.451038	50.409268
247.330389	139.183400	50.414273
243.644609	138.948840	50.419277
240.430892	134.424047	50.424282
236.634764	136.227373	50.429287
232.798802	139.758503	50.434292
229.450255	131.073842	50.439297
226.174687	130.698119	50.444301
222.959486	127.958436	50.449306
219.206443	131.659961	50.454311
215.261777	137.045805	50.459316
212.352278	135.482186	50.464321
208.467506	137.595446	50.469325
204.785248	124.323765	50.474330
201.736759	137.221849	50.479335
198.178465	144.582064	50.484340
194.707693	131.164753	50.489345
191.493309	131.761140	50.494349
187.629225	132.215181	50.499354
183.762546	137.373190	50.504359
180.384597	140.439779	50.509364
177.256962	131.156124	50.514369
173.493056	141.306523	50.519373
169.997003	125.664614	50.524378
166.547766	139.696561	50.529383
163.143517	128.876601	50.534388
159.948820	134.466584	50.539393
155.737168	142.069435	50.544397
152.621122	134.151915	50.549402
148.987761	132.783006	50.554407
145.203211	137.390788	50.559412
142.002381	132.458157	50.564417
138.417098	125.785952	50.569421
135.473073	142.351631	50.574426
131.688206	129.971423	50.579431
127.960478	141.381895	50.584436
124.812312	128.020934	50.589441
120.951098	137.284749	50.594445
117.499008	133.934428	50.599450
113.890197	126.735762	50.604455
110.155468	129.342713	50.609460
107.217014	134.201181	50.614465
103.583889	142.094798	50.619469
100.314019	124.894122	50.624474
96.286174	126.883994	50.629479
92.768633	138.040046	50.634484
89.221869	137.595260	50.639489
85.753308	135.541824	50.644493
82.630909	127.187868	50.649498
79.460993	127.578669	50.654503
75.654543	136.829511	50.659508
72.117780	139.524822	50.664513
68.138475	135.351465	50.669517
64.755655	128.625626	50.674522
61.378769	120.367110	50.679527
57.687422	133.350751	50.684532
54.708054	121.284603	50.689537
51.124457	125.074138	50.694541
47.355838	123.539211	50.699546
43.944733	126.231824	50.704551
40.068159	130.353804	50.709556
36.867654	129.676029	50.714561
33.476785	136.087718	50.719565
30.196210	126.276076	50.724570
26.683296	120.170197	50.729575
22.877190	128.923000	50.734580
19.111314	132.334149	50.739585
16.144481	123.086568	50.744589
12.436627	123.070265	50.749594
9.194846	131.520082	50.754599
5.068098	125.306407	50.759604
1.912204	124.382634	50.764609