Thu Jun 16 11:37:56 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.451820	94.590121	0.000000
0.682391	106.912381	0.005005
0.788806	107.516946	0.010010
0.421970	114.717775	0.015014
0.336527	91.718094	0.020019
0.216046	83.436047	0.025024
0.464252	71.597584	0.030029
-0.093901	68.443769	0.035034
-0.302778	63.646774	0.040038
-0.364206	48.063511	0.045043
-0.691194	41.572629	0.050048
-1.600585	20.667981	0.055053
-1.403471	20.052111	0.060058
-2.275701	20.861710	0.065062
-2.503263	3.453734	0.070067
-3.121187	15.101167	0.075072
-3.344585	0.977657	0.080077
-2.943984	-2.933508	0.085082
-3.192184	6.772098	0.090086
-3.603095	-1.083474	0.095091
-4.060285	8.747332	0.100096
-4.674230	5.743035	0.105101
-4.397778	1.932098	0.110106
-4.889732	8.486758	0.115110
-5.376435	3.889692	0.120115
-5.781383	7.790609	0.125120
-6.196102	-0.680619	0.130125
-6.177877	1.813122	0.135130
-6.377912	6.330101	0.140134
-6.088677	-0.547212	0.145139
-6.122947	6.989668	0.150144
-6.478965	0.699034	0.155149
-6.843502	9.236676	0.160154
-7.828957	10.272553	0.165158
-7.889070	-4.421515	0.170163
-8.004340	10.424737	0.175168
-7.847492	7.822827	0.180173
-7.799472	-3.174822	0.185178
-8.693519	4.843016	0.190182
-9.157040	6.381597	0.195187
-9.251556	0.654465	0.200192
-9.505292	16.204212	0.205197
-9.351232	10.470328	0.210202
-9.523067	5.197149	0.215206
-10.291826	17.144851	0.220211
-10.897789	12.951648	0.225216
-11.148606	0.422860	0.230221
-11.013415	1.217702	0.235226
-11.180068	0.882142	0.240230
-11.013137	-3.572656	0.245235
-11.262342	0.639618	0.250240
-11.594346	12.333025	0.255245
-12.234230	6.788949	0.260250
-12.786012	8.113242	0.265254
-12.664215	-0.213730	0.270259
-12.597469	-1.542034	0.275264
-12.431058	0.542964	0.280269
-13.863553	0.542280	0.285274
-14.460636	9.129007	0.290278
-14.280869	0.246311	0.295283
-14.210672	7.116690	0.300288
-14.459421	-2.142580	0.305293
-14.279677	-8.114213	0.310298
-14.381941	9.091542	0.315302
-14.802127	-5.130550	0.320307
-15.344081	1.456441	0.325312
-15.496450	4.103466	0.330317
-15.849693	-1.884562	0.335322
-16.220369	15.024513	0.340326
-16.044420	3.291963	0.345331
-17.099326	3.496625	0.350336
-17.718889	-2.433382	0.355341
-17.647753	0.774543	0.360346
-18.006024	-7.498639	0.365350
-17.956662	-1.032751	0.370355
-17.921591	-0.087984	0.375360
-17.876044	-1.907825	0.380365
-17.933219	-6.020157	0.385370
-18.048452	-3.370195	0.390374
-18.342063	-9.227099	0.395379
-18.814112	19.339296	0.400384
-19.396565	13.139451	0.405389
-19.505135	0.581041	0.410394
-20.602911	2.472158	0.415398
-20.889491	7.389469	0.420403
-20.612748	3.738203	0.425408
-20.621466	1.014887	0.430413
-20.934245	8.542744	0.435418
-21.064362	2.737838	0.440422
-21.092484	4.479214	0.445427
-21.101385	4.271976	0.450432
-22.020970	11.128057	0.455437
-22.412017	2.977980	0.460442
-22.821772	17.738143	0.465446
-22.771494	5.231414	0.470451
-22.774006	-1.778317	0.475456
-23.007364	6.261544	0.480461
-22.892695	-0.866107	0.485466
-23.845038	-1.906329	0.490470
-23.994150	0.293259	0.495475
-24.317731	-6.494713	0.500480
-24.533374	5.079720	0.505485
-24.342971	-0.433066	0.510490
-24.875330	-0.026003	0.515494
-25.170896	-3.542536	0.520499
-25.423028	-7.010506	0.525504
-25.660422	4.272843	0.530509
-25.441664	-1.684917	0.535514
-26.248235	-1.709525	0.540518
-26.873691	0.062892	0.545523
-27.115135	8.854840	0.550528
-27.075049	0.918622	0.555533
-27.059595	-1.663668	0.560538
-27.427509	5.023305	0.565542
-27.450050	-7.123233	0.570547
-27.503252	0.651861	0.575552
-28.255959	2.786055	0.580557
-28.259863	-10.105234	0.585562
-28.911267	0.303115	0.590566
-28.862838	-5.569474	0.595571
-28.918128	1.854169	0.600576
-29.438742	11.660140	0.605581
-29.692069	2.658420	0.610586
-30.359891	5.663308	0.615590
-30.611943	-3.029441	0.620595
-30.413305	4.544020	0.625600
-30.494414	16.243022	0.630605
-30.313756	0.870976	0.635610
-31.099794	10.049674	0.640614
-31.874898	17.374062	0.645619
-31.807530	5.502104	0.650624
-32.086070	11.051736	0.655629
-31.970888	6.013766	0.660634
-32.308363	3.998851	0.665638
-32.468619	-4.079167	0.670643
-32.993488	9.952913	0.675648
-33.246783	6.985698	0.680653
-33.450310	-4.577388	0.685658
-33.804232	4.586323	0.690662
-33.713275	5.882826	0.695667
-33.907922	-0.912742	0.700672
-35.019638	-10.364216	0.705677
-34.812966	-6.020013	0.710682
-35.384655	10.233479	0.715686
-35.241469	8.474648	0.720691
-35.375223	0.525528	0.725696
-35.525404	8.195407	0.730701
-35.348022	-4.140043	0.735706
-36.484769	14.119619	0.740710
-36.506577	8.217495	0.745715
-36.554861	8.545053	0.750720
-36.866652	-1.684802	0.755725
-36.374365	7.527492	0.760730
-37.584400	0.663456	0.765734
-37.837224	6.900591	0.770739
-38.032200	2.529870	0.775744
-38.147951	0.871840	0.780749
-38.035416	-8.154328	0.785754
-38.859676	10.403709	0.790758
-39.638897	-8.587515	0.795763
-39.487468	-5.579907	0.800768
-39.699728	12.084707	0.805773
-39.346042	-1.746557	0.810778
-39.798023	5.769578	0.815782
-39.643413	-9.147999	0.820787
-40.449322	-3.359982	0.825792
-41.571693	-1.716855	0.830797
-41.301096	3.573522	0.835802
-41.838467	10.056766	0.840806
-41.556167	2.410316	0.845811
-41.382837	1.320008	0.850816
-41.526330	7.175736	0.855821
-41.434767	3.391407	0.860826
-42.277531	10.692742	0.865830
-42.817501	12.488225	0.870835
-43.339549	0.556627	0.875840
-43.370620	12.206315	0.880845
-43.057213	13.362667	0.885850
-43.539360	8.104173	0.890854
-44.305529	5.490548	0.895859
-44.624524	7.159146	0.900864
-44.741717	10.248440	0.905869
-45.015157	6.184771	0.910874
-45.057544	4.612874	0.915878
-44.576181	-0.346805	0.920883
-44.901238	18.178855	0.925888
-46.063428	5.719890	0.930893
-46.001144	3.462519	0.935898
-46.583740	6.890553	0.940902
-46.681050	4.469551	0.945907
-46.235184	2.462898	0.950912
-46.815471	17.736714	0.955917
-47.578414	-2.527561	0.960922
-48.204773	4.886776	0.965926
-47.805882	7.560883	0.970931
-48.181455	9.299405	0.975936
-48.609265	-1.234067	0.980941
-48.100476	2.421627	0.985946
-48.640345	-0.063856	0.990950
-48.674116	10.883868	0.995955
-48.654294	3.278132	1.000960
-49.594164	-8.449745	1.005965
-49.477422	1.072423	1.010970
-49.851833	21.511529	1.015974
-50.333932	-1.689993	1.020979
-50.987085	11.815370	1.025984
-51.191213	7.908449	1.030989
-50.882809	2.559064	1.035994
-51.258847	9.166683	1.040998
-51.340201	7.825860	1.046003
-51.272144	-2.543322	1.051008
-51.825910	4.857241	1.056013
-52.247040	-1.717893	1.061018
-52.879839	7.487370	1.066022
-52.866192	-0.030331	1.071027
-52.634012	9.740113	1.076032
-53.033658	3.859100	1.081037
-53.120987	-4.408740	1.086042
-54.010296	2.542962	1.091046
-54.439564	5.111150	1.096051
-54.725158	3.504669	1.101056
-54.698953	20.428162	1.106061
-54.374382	-3.033441	1.111066
-54.642031	4.928724	1.116070
-55.146398	16.444925	1.121075
-56.047674	-0.005841	1.126080
-56.397455	6.149355	1.131085
-55.710639	2.765442	1.136090
-56.322038	18.242297	1.141094
-56.535339	1.395584	1.146099
-56.476241	6.835254	1.151104
-56.820115	6.598830	1.156109
-56.785431	6.200302	1.161114
-57.940458	12.418833	1.166118
-57.847985	9.800235	1.171123
-58.442658	-0.054351	1.176128
-58.322272	5.855235	1.181133
-58.234335	1.159953	1.186138
-58.613928	6.466333	1.191142
-58.529505	4.217930	1.196147
-59.178791	-6.308135	1.201152
-59.522450	11.676321	1.206157
-59.867332	7.223238	1.211162
-60.088095	11.599511	1.216166
-60.022702	3.663255	1.221171
-60.851985	2.184215	1.226176
-61.597109	8.715507	1.231181
-61.071336	-3.833983	1.236186
-61.296366	10.843454	1.241190
-61.289717	15.526050	1.246195
-61.457916	1.627333	1.251200
-61.400987	17.702063	1.256205
-62.088480	3.717413	1.261210
-62.870166	0.771133	1.266214
-63.025300	-8.308363	1.271219
-63.182255	1.030556	1.276224
-63.156742	1.101751	1.281229
-63.020259	-3.960650	1.286234
-63.862048	1.705841	1.291238
-64.269660	4.417937	1.296243
-64.228594	-2.455946	1.301248
-64.340093	3.533297	1.306253
-64.517032	-0.314286	1.311258
-65.070583	1.711331	1.316262
-65.869115	-6.372871	1.321267
-66.088538	-3.057046	1.326272
-66.246977	-7.445442	1.331277
-66.015839	-5.392257	1.336282
-66.322627	2.452466	1.341286
-66.238090	-2.851731	1.346291
-66.343973	-0.574643	1.351296
-66.628276	4.522924	1.356301
-67.174565	-7.641720	1.361306
-67.783183	0.487778	1.366310
-68.177410	10.739488	1.371315
-68.321529	-0.640153	1.376320
-68.045886	2.052940	1.381325
-68.299194	1.102691	1.386330
-68.683703	-4.327607	1.391334
-69.212721	-2.378949	1.396339
-69.235822	-0.562441	1.401344
-69.433351	9.217360	1.406349
-69.718923	-6.765429	1.411354
-69.807366	0.090812	1.416358
-70.188641	4.150199	1.421363
-70.595780	-9.811615	1.426368
-70.994297	-3.276151	1.431373
-70.835245	-0.355928	1.436378
-71.071161	-3.043271	1.441382
-71.004289	2.436447	1.446387
-71.924373	3.426014	1.451392
-72.683384	-2.167714	1.456397
-72.817076	0.062374	1.461402
-72.561120	-1.304204	1.466406
-72.534133	-3.787871	1.471411
-72.885379	4.318626	1.476416
-73.282470	-5.361338	1.481421
-73.769755	-5.899417	1.486426
-73.951341	12.649480	1.491430
-74.545161	-0.008964	1.496435
-74.710411	-4.290873	1.501440
-74.458831	7.999115	1.506445
-74.555212	-0.598507	1.511450
-74.526130	3.649460	1.516454
-75.259377	7.297431	1.521459
-75.739545	-3.057303	1.526464
-75.900286	-1.707169	1.531469
-75.937578	-0.119361	1.536474
-76.101779	1.999655	1.541478
-76.269430	3.274082	1.546483
-76.565255	6.999416	1.551488
-77.359079	9.442487	1.556493
-77.073780	2.276674	1.561498
-77.634947	18.458980	1.566502
-77.429051	3.445514	1.571507
-77.709106	4.052583	1.576512
-79.197680	9.959252	1.581517
-79.461480	7.993131	1.586522
-78.766901	8.365034	1.591526
-79.051762	12.422006	1.596531
-78.866544	16.591688	1.601536
-79.666802	18.572845	1.606541
-79.396740	-1.305051	1.611546
-80.353471	1.269712	1.616550
-80.605627	6.911267	1.621555
-80.728144	6.600082	1.626560
-81.208464	8.643884	1.631565
-81.051491	4.791626	1.636570
-80.914478	14.884412	1.641574
-81.064496	12.139660	1.646579
-81.482928	3.505784	1.651584
-82.533762	8.703796	1.656589
-82.588781	4.875623	1.661594
-82.555889	11.657260	1.666598
-83.005606	15.596162	1.671603
-82.749386	1.983245	1.676608
-82.996256	16.556763	1.681613
-83.299879	8.785276	1.686618
-83.982844	5.972143	1.691622
-83.693303	9.620169	1.696627
-84.159917	0.177214	1.701632
-85.036569	9.289697	1.706637
-84.999797	-1.631405	1.711642
-85.461121	4.245576	1.716646
-85.611820	4.136552	1.721651
-85.745718	6.373975	1.726656
-86.231581	13.003495	1.731661
-85.950365	1.455301	1.736666
-85.777469	16.614104	1.741670
-85.906174	4.593728	1.746675
-86.636574	-5.586662	1.751680
-87.118077	8.819836	1.756685
-87.221074	5.784476	1.761690
-87.450342	3.286138	1.766694
-87.726136	2.256442	1.771699
-88.353443	-2.092641	1.776704
-88.807672	12.860823	1.781709
-88.764073	12.365720	1.786714
-89.300895	15.687737	1.791718
-89.130632	6.708848	1.796723
-88.928047	0.526169	1.801728
-89.257680	7.573805	1.806733
-89.457479	2.612164	1.811738
-90.342480	6.200572	1.816742
-90.756629	16.357615	1.821747
-90.543577	1.663789	1.826752
-90.883937	8.351438	1.831757
-90.674037	-8.916405	1.836762
-90.767022	1.961383	1.841766
-91.852207	3.051243	1.846771
-91.907238	-10.022678	1.851776
-92.629899	-2.168615	1.856781
-92.138895	-10.434957	1.861786
-92.188255	-1.103070	1.866790
-92.828300	-2.424066	1.871795
-93.136705	6.024188	1.876800
-93.639670	-0.069505	1.881805
-94.010158	-4.605362	1.886810
-94.416588	-2.934052	1.891814
-94.239591	-4.868647	1.896819
-94.023258	-5.047013	1.901824
-94.100208	10.297503	1.906829
-94.515097	0.818378	1.911834
-95.369936	8.917544	1.916838
-95.416400	-5.309373	1.921843
-95.310218	-1.567711	1.926848
-95.821065	4.929793	1.931853
-95.716214	-1.136303	1.936858
-96.478088	7.358584	1.941862
-97.303862	3.070418	1.946867
-96.864512	4.663503	1.951872
-97.380624	6.044058	1.956877
-97.252654	-4.375271	1.961882
-97.383581	-4.069077	1.966886
-97.352202	0.208204	1.971891
-98.287928	-2.046013	1.976896
-98.608224	20.598603	1.981901
-98.776973	-1.354444	1.986906
-98.807511	2.150456	1.991910
-99.015442	9.207475	1.996915
-99.078942	-2.595796	2.006912
-99.130497	-0.205923	2.016909
-98.957842	1.944991	2.026906
-98.198022	2.651957	2.036902
-97.722733	8.926477	2.046899
-97.155468	5.109812	2.056896
-96.228119	1.886468	2.066893
-96.112703	10.136982	2.076890
-95.619187	2.883133	2.086886
-94.702032	1.999531	2.096883
-94.605777	6.328017	2.106880
-94.448011	6.407373	2.116877
-93.388509	5.833872	2.126874
-93.064945	4.598977	2.136870
-92.909116	2.496272	2.146867
-92.071084	1.210084	2.156864
-91.626112	-3.188476	2.166861
-90.912944	1.058746	2.176858
-90.123384	-1.323141	2.186854
-90.002203	1.078437	2.196851
-89.983055	3.850113	2.206848
-88.952344	6.304315	2.216845
-88.866657	5.530177	2.226842
-87.918835	6.553431	2.236838
-87.049138	5.644533	2.246835
-87.192693	5.671698	2.256832
-86.967286	7.589072	2.266829
-85.594187	8.390019	2.276826
-85.364728	9.290285	2.286822
-85.544946	9.508819	2.296819
-84.717548	-1.848729	2.306816
-84.190532	0.025416	2.316813
-82.971210	1.226496	2.326810
-82.952285	3.696785	2.336806
-82.636234	6.197485	2.346803
-82.252054	0.508739	2.356800
-81.366691	-1.374142	2.366797
-80.901883	2.933735	2.376794
-81.110972	3.051100	2.386790
-79.797220	8.405409	2.396787
-79.067304	3.033452	2.406784
-78.853265	10.670053	2.416781
-79.033906	4.799208	2.426778
-77.972828	4.543321	2.436774
-77.797727	5.901325	2.446771
-76.657879	-0.092977	2.456768
-76.099576	6.896224	2.466765
-76.141964	-2.053849	2.476762
-76.028484	-2.368366	2.486758
-75.114036	-4.431239	2.496755
-74.841738	0.384275	2.506752
-73.849658	1.028114	2.516749
-73.147286	-2.252230	2.526746
-73.111250	3.413753	2.536742
-72.627407	-0.925197	2.546739
-71.533133	8.585225	2.556736
-71.243514	1.563917	2.566733
-71.472745	5.621164	2.576730
-70.544919	6.687484	2.586726
-70.175951	5.527469	2.596723
-69.377792	-1.417763	2.606720
-68.745572	-0.784434	2.616717
-68.622704	1.324776	2.626714
-67.976716	2.223373	2.636710
-67.142152	3.497281	2.646707
-67.086154	0.682479	2.656704
-66.521532	1.664262	2.666701
-66.169040	-0.121267	2.676698
-65.507809	-0.542608	2.686694
-64.980894	6.056220	2.696691
-64.353640	-2.723645	2.706688
-63.568024	4.577866	2.716685
-63.498788	1.867113	2.726682
-63.523575	1.125359	2.736678
-62.620853	3.172361	2.746675
-62.087549	8.743472	2.756672
-61.135476	3.233453	2.766669
-60.680096	6.228583	2.776666
-60.474291	10.697065	2.786662
-60.428107	-3.808971	2.796659
-59.592689	5.509236	2.806656
-58.941984	4.432308	2.816653
-58.080795	-1.283264	2.826650
-57.677754	-2.502448	2.836646
-57.475626	2.101226	2.846643
-57.346789	9.260632	2.856640
-56.261496	1.323615	2.866637
-55.874098	0.769875	2.876634
-55.779051	3.762376	2.886630
-54.776471	4.989701	2.896627
-53.775231	5.695249	2.906624
-53.866096	4.576854	2.916621
-53.799238	-4.766685	2.926618
-53.498685	-2.704324	2.936614
-52.879698	4.305571	2.946611
-51.798521	5.209592	2.956608
-51.146221	1.120718	2.966605
-51.155998	0.677513	2.976602
-50.088686	9.803305	2.986598
-49.629523	6.151986	2.996595
-49.663401	6.379920	3.006592
-49.310393	7.386997	3.016589
-48.217725	-0.764551	3.026586
-47.865302	6.574872	3.036582
-47.851705	5.601656	3.046579
-46.898264	-0.260834	3.056576
-46.352194	3.966646	3.066573
-46.026235	-3.000312	3.076570
-44.766002	1.280770	3.086566
-44.665870	2.338578	3.096563
-44.607823	1.229800	3.106560
-44.333624	4.520098	3.116557
-43.488611	0.701047	3.126554
-43.021951	3.000538	3.136550
-42.095172	9.729415	3.146547
-41.582582	6.457271	3.156544
-41.393828	6.388721	3.166541
-41.103519	8.321104	3.176538
-40.741366	10.543040	3.186534
-40.084720	1.214041	3.196531
-39.329235	2.808177	3.206528
-38.512881	4.999845	3.216525
-38.475860	7.265536	3.226522
-38.190197	5.043928	3.236518
-37.429513	4.212715	3.246515
-36.749365	1.864325	3.256512
-36.404560	7.979108	3.266509
-36.005628	6.663158	3.276506
-35.177831	7.064832	3.286502
-35.128025	5.644433	3.296499
-34.446355	7.886267	3.306496
-33.522625	4.102263	3.316493
-33.037060	5.486256	3.326490
-32.922638	1.387148	3.336486
-32.637294	1.423245	3.346483
-31.563613	1.555017	3.356480
-31.626515	-2.899085	3.366477
-31.251835	-0.103140	3.376474
-30.340845	-0.400742	3.386470
-30.219206	-2.789245	3.396467
-29.150549	10.580880	3.406464
-28.433096	14.495804	3.416461
-28.273932	0.868005	3.426458
-28.014681	6.518835	3.436454
-27.865806	0.478353	3.446451
-26.983760	5.650996	3.456448
-26.153757	2.458071	3.466445
-25.279937	4.422189	3.476442
-25.416262	6.059695	3.486438
-25.451014	2.003217	3.496435
-24.440808	-0.850843	3.506432
-23.847580	-0.424281	3.516429
-23.620886	3.511736	3.526426
-22.425959	-1.518635	3.536422
-22.224266	11.330279	3.546419
-22.300339	7.140363	3.556416
-21.264013	7.311401	3.566413
-20.872690	6.053458	3.576410
-20.588571	2.692883	3.586406
-19.401524	7.553161	3.596403
-19.245713	4.298493	3.606400
-19.324210	-4.864512	3.616397
-18.765005	6.807036	3.626394
-17.877935	11.000887	3.636390
-17.205015	3.556082	3.646387
-16.385991	7.627332	3.656384
-15.945952	1.077432	3.666381
-15.980208	-1.653409	3.676378
-15.641651	5.030241	3.686374
-14.909126	0.761569	3.696371
-14.699415	3.877709	3.706368
-13.562927	-3.588533	3.716365
-12.720527	10.066677	3.726362
-12.660887	8.800675	3.736358
-12.514172	-5.152073	3.746355
-12.278982	8.503370	3.756352
-11.304851	-0.077291	3.766349
-10.760622	2.152339	3.776346
-10.262078	1.897168	3.786342
-9.489520	2.154026	3.796339
-9.363756	0.259973	3.806336
-9.187182	3.175388	3.816333
-7.928909	3.478762	3.826330
-7.620645	1.501701	3.836326
-7.605852	9.925863	3.846323
-7.272870	9.234579	3.856320
-6.168667	9.784532	3.866317
-5.788364	-1.136313	3.876314
-5.711785	9.712105	3.886310
-5.118917	11.744883	3.896307
-4.276299	21.292870	3.906304
-3.761924	23.650615	3.916301
-3.769846	29.677311	3.926298
-3.057684	38.891212	3.936294
-2.725650	47.652802	3.946291
-2.185788	54.461503	3.956288
-1.548388	67.793409	3.966285
-1.206572	76.465386	3.976282
-0.951792	91.676118	3.986278
-0.272121	115.242343	3.996275
0.000000	127.293425	4.001280
0.027757	139.325248	4.006285
0.336059	140.344143	4.011290
0.651937	159.621463	4.016294
0.952671	169.870505	4.021299
1.403734	156.660901	4.026304
1.245523	160.783106	4.031309
1.044577	145.563946	4.036314
1.071682	171.373925	4.041318
0.788110	165.923720	4.046323
1.166144	148.577983	4.051328
0.949368	160.861058	4.056333
0.914599	154.124825	4.061338
0.884150	159.386581	4.066342
0.900663	166.074516	4.071347
1.008730	168.332944	4.076352
0.837918	165.968751	4.081357
0.608500	164.794739	4.086362
0.780217	179.642760	4.091366
0.900436	165.726606	4.096371
1.127219	168.443297	4.101376
0.459994	170.679795	4.106381
1.201963	169.446769	4.111386
1.095947	162.588631	4.116390
0.907262	161.086571	4.121395
0.957223	166.334843	4.126400
1.158512	178.902815	4.131405
1.136491	178.749240	4.136410
1.456436	202.096315	4.141414
1.228133	190.600014	4.146419
1.073274	166.621499	4.151424
0.862050	175.929247	4.156429
1.430280	185.028279	4.161434
1.348605	196.924627	4.166438
1.708076	189.800628	4.171443
1.515473	174.730015	4.176448
1.136988	174.001101	4.181453
1.395825	168.116758	4.186458
1.026073	174.619329	4.191462
1.337556	167.944354	4.196467
0.938410	169.103740	4.201472
1.112681	180.721699	4.206477
1.451945	185.030334	4.211482
1.342437	190.497936	4.216486
1.352501	191.609628	4.221491
1.420190	182.467143	4.226496
1.420791	198.235392	4.231501
1.429829	197.064886	4.236506
1.576484	199.688277	4.241510
1.350813	201.467847	4.246515
1.454922	191.818174	4.251520
1.406145	193.516815	4.256525
1.236985	191.526147	4.261530
1.154918	191.866197	4.266534
1.524633	183.609732	4.271539
1.101691	194.924873	4.276544
1.217913	197.935579	4.281549
1.284890	196.266665	4.286554
1.315664	206.286580	4.291558
1.600867	226.959192	4.296563
1.456783	226.942200	4.301568
1.521596	230.470071	4.306573
1.559659	234.562425	4.311578
1.368461	225.036312	4.316582
1.665857	224.358481	4.321587
1.732586	231.058370	4.326592
1.742477	229.874500	4.331597
1.928899	214.771202	4.336602
1.729764	220.147079	4.341606
1.487604	226.128211	4.346611
1.979230	221.804074	4.351616
1.595997	225.708757	4.356621
2.111736	214.264295	4.361626
1.911328	229.883679	4.366630
1.618916	234.306780	4.371635
1.661636	211.838797	4.376640
1.608121	226.469655	4.381645
1.558539	225.870671	4.386650
1.841755	233.248451	4.391654
2.124550	224.320581	4.396659
2.337479	223.409875	4.401664
1.900344	222.653260	4.406669
1.756989	201.068418	4.411674
1.702563	215.482475	4.416678
1.896659	220.724408	4.421683
2.198881	218.490097	4.426688
1.813055	227.921537	4.431693
2.055679	234.775758	4.436698
1.927311	230.130356	4.441702
2.100402	231.386768	4.446707
2.222066	214.963519	4.451712
1.920589	205.943884	4.456717
1.759722	200.659155	4.461722
1.733370	228.171367	4.466726
1.600516	214.975734	4.471731
2.102320	220.489219	4.476736
1.839940	235.682009	4.481741
1.982504	229.158240	4.486746
1.783462	228.319561	4.491750
1.941745	229.951433	4.496755
2.096353	221.804585	4.501760
2.049389	218.836080	4.506765
2.243782	222.349145	4.511770
2.123542	224.892342	4.516774
2.262956	230.494526	4.521779
2.053903	233.313244	4.526784
1.744960	248.395257	4.531789
2.031354	232.733115	4.536794
2.144442	231.541465	4.541798
2.147627	243.396498	4.546803
1.822205	235.165304	4.551808
1.961592	237.290612	4.556813
2.333791	256.606890	4.561818
2.647144	254.456564	4.566822
2.487799	256.137673	4.571827
2.333624	238.796126	4.576832
2.029106	232.465217	4.581837
2.256886	225.358624	4.586842
2.124876	244.136193	4.591846
2.448275	259.696471	4.596851
2.863755	249.887672	4.601856
2.198680	243.740944	4.606861
2.430135	239.062022	4.611866
2.045053	232.018033	4.616870
2.053049	240.418373	4.621875
2.274149	249.189663	4.626880
2.108744	254.619171	4.631885
2.457025	246.547147	4.636890
2.522915	253.559426	4.641894
2.554965	260.687103	4.646899
2.535704	260.507816	4.651904
2.652565	265.749605	4.656909
2.492799	247.287465	4.661914
2.888716	256.247994	4.666918
2.648134	265.589948	4.671923
2.733157	258.960545	4.676928
2.404127	252.998109	4.681933
2.730787	255.303987	4.686938
2.369266	247.093057	4.691942
2.709002	244.935314	4.696947
2.824521	244.855789	4.701952
2.434217	244.123892	4.706957
2.513436	235.737630	4.711962
2.533888	256.280994	4.716966
2.898944	246.455473	4.721971
2.884506	247.920751	4.726976
2.346711	237.571613	4.731981
2.800822	245.007973	4.736986
2.741011	248.714388	4.741990
2.590076	260.354976	4.746995
2.806750	254.731209	4.752000
2.523913	254.556610	4.757005
2.780552	257.441719	4.762010
2.698825	265.578694	4.767014
2.753817	265.124122	4.772019
2.847270	265.225723	4.777024
2.942394	267.272521	4.782029
3.013377	267.848222	4.787034
2.884356	267.068310	4.792038
2.668145	254.832024	4.797043
2.645269	249.579622	4.802048
2.834848	261.666189	4.807053
2.401039	260.985974	4.812058
2.303189	265.095173	4.817062
2.457747	268.534625	4.822067
2.724998	277.723703	4.827072
2.311688	271.882030	4.832077
2.835925	280.498865	4.837082
2.986817	298.765973	4.842086
2.835697	295.978926	4.847091
2.862015	293.886684	4.852096
2.766903	299.282887	4.857101
3.059547	295.575749	4.862106
2.758604	313.241757	4.867110
2.835956	305.126279	4.872115
2.754906	289.216900	4.877120
2.676892	313.469661	4.882125
2.827720	296.024274	4.887130
3.022399	302.941794	4.892134
3.161387	305.034622	4.897139
3.220427	298.766233	4.902144
2.974718	292.853643	4.907149
3.066572	296.338585	4.912154
2.862107	314.585414	4.917158
3.171274	302.471121	4.922163
3.260271	310.284138	4.927168
2.795460	309.253491	4.932173
3.399949	312.663881	4.937178
3.202985	321.464246	4.942182
2.968393	317.893560	4.947187
3.467193	319.971323	4.952192
3.079306	321.969499	4.957197
3.541898	320.876354	4.962202
3.521738	308.630119	4.967206
3.136575	310.817657	4.972211
2.942844	293.296029	4.977216
2.779781	322.032717	4.982221
3.247301	326.421517	4.987226
3.342965	326.050984	4.992230
3.169965	325.081422	4.997235
3.666763	326.676204	5.002240
3.498711	338.351249	5.007245
3.516369	323.320129	5.012250
3.823477	331.594434	5.017254
3.685335	325.608809	5.022259
3.531888	302.845872	5.027264
3.070394	307.178451	5.032269
3.331259	306.859246	5.037274
3.344651	308.684560	5.042278
3.145873	325.988702	5.047283
3.389406	327.470154	5.052288
3.442833	331.943665	5.057293
3.491123	321.020026	5.062298
3.394854	332.324888	5.067302
3.197122	327.261375	5.072307
3.846931	322.757858	5.077312
3.537671	344.869789	5.082317
3.763998	331.816646	5.087322
3.590889	327.972092	5.092326
3.530918	326.966191	5.097331
3.804634	339.151678	5.102336
3.559532	334.556809	5.107341
3.546300	330.678533	5.112346
3.573024	338.362061	5.117350
3.635446	334.801876	5.122355
3.554216	324.280941	5.127360
3.433219	326.849141	5.132365
3.371212	341.717198	5.137370
3.688192	324.961643	5.142374
3.304570	323.534598	5.147379
3.593532	324.448872	5.152384
3.297967	330.128105	5.157389
3.576915	314.402986	5.162394
3.759808	339.979341	5.167398
3.708654	353.430506	5.172403
4.152077	344.454120	5.177408
4.103854	343.872665	5.182413
3.829777	329.942598	5.187418
3.950133	329.410828	5.192422
3.749586	336.124250	5.197427
3.885292	336.955330	5.202432
3.547122	337.963279	5.207437
3.552992	331.359850	5.212442
3.756977	360.790172	5.217446
3.911822	360.920006	5.222451
4.165955	358.013492	5.227456
3.854288	362.829205	5.232461
4.206408	364.133289	5.237466
3.912113	352.219212	5.242470
3.845732	363.003585	5.247475
4.115927	366.934885	5.252480
3.988374	376.400587	5.257485
4.199977	359.276961	5.262490
3.949168	349.739609	5.267494
3.466261	354.381768	5.272499
3.864221	355.133995	5.277504
3.977552	361.410308	5.282509
4.109045	369.263984	5.287514
4.046589	372.661384	5.292518
3.867056	363.362731	5.297523
4.087930	368.003128	5.302528
3.895752	376.744527	5.307533
4.174528	370.073784	5.312538
3.893413	369.204660	5.317542
3.656522	367.038012	5.322547
4.001028	361.972386	5.327552
3.818459	373.740028	5.332557
4.065552	361.837203	5.337562
4.090734	369.939005	5.342566
4.280115	383.288392	5.347571
4.463317	397.046949	5.352576
4.012290	396.069166	5.357581
4.439460	392.214284	5.362586
4.391140	387.303541	5.367590
4.280179	380.421458	5.372595
4.187213	375.369818	5.377600
4.356159	379.874073	5.382605
4.180559	382.361135	5.387610
4.330923	389.599940	5.392614
4.293121	393.053648	5.397619
4.568904	392.357184	5.402624
4.351983	394.782017	5.407629
4.440933	378.526782	5.412634
4.595534	381.264910	5.417638
4.125493	372.484649	5.422643
4.248298	375.278049	5.427648
4.360644	398.234130	5.432653
4.632678	388.828379	5.437658
4.543848	391.579015	5.442662
4.440507	400.330312	5.447667
4.588921	391.340104	5.452672
4.556223	388.657874	5.457677
4.591973	386.822045	5.462682
4.477122	375.121976	5.467686
4.361300	367.292228	5.472691
4.779028	376.625989	5.477696
4.457990	391.800608	5.482701
4.891956	372.854455	5.487706
4.518430	368.277544	5.492710
4.728664	374.012804	5.497715
4.402236	368.737817	5.502720
4.359566	361.820286	5.507725
4.848598	373.588323	5.512730
4.490623	381.740132	5.517734
4.468741	385.370859	5.522739
4.719743	396.163578	5.527744
4.345055	395.584079	5.532749
4.202963	389.827963	5.537754
4.959869	401.478847	5.542758
4.549969	392.860691	5.547763
5.252424	387.415568	5.552768
4.735904	401.892845	5.557773
4.930687	400.185426	5.562778
4.820091	393.068575	5.567782
4.971712	401.281401	5.572787
5.091398	389.456830	5.577792
4.752927	379.725092	5.582797
4.396046	362.718296	5.587802
4.656137	388.834840	5.592806
4.571062	397.887074	5.597811
4.662596	394.822840	5.602816
4.798476	397.629868	5.607821
4.831987	399.186878	5.612826
4.678921	402.063165	5.617830
4.941396	399.629305	5.622835
5.049025	397.917741	5.627840
4.955852	405.650221	5.632845
5.048959	401.322439	5.637850
4.941825	397.273994	5.642854
4.931561	406.004782	5.647859
4.977739	392.526259	5.652864
4.798494	398.776552	5.657869
4.855434	398.727918	5.662874
4.870679	402.700472	5.667878
4.631758	407.763049	5.672883
4.916757	404.934790	5.677888
5.167872	395.252210	5.682893
4.825417	393.316396	5.687898
4.784902	402.638984	5.692902
5.028846	420.288666	5.697907
5.054028	423.913795	5.702912
4.959668	430.565906	5.707917
5.601632	428.687901	5.712922
5.255451	424.722460	5.717926
5.261824	423.271997	5.722931
5.036856	397.121653	5.727936
4.815269	411.252358	5.732941
5.060134	431.342445	5.737946
5.222267	432.742551	5.742950
5.051503	434.136110	5.747955
5.339472	435.601449	5.752960
5.173450	441.160068	5.757965
5.486442	435.727002	5.762970
5.562814	431.016924	5.767974
5.417509	432.044702	5.772979
5.377091	427.789885	5.777984
5.419352	418.488779	5.782989
5.274646	402.781589	5.787994
5.120871	404.334034	5.792998
4.905252	425.888001	5.798003
5.454700	419.820379	5.803008
5.526695	427.336944	5.808013
5.619810	424.596625	5.813018
5.423689	428.598295	5.818022
5.150600	443.543756	5.823027
5.180162	422.627129	5.828032
5.284945	430.983561	5.833037
5.209378	440.016687	5.838042
5.654368	429.791602	5.843046
5.188698	427.492472	5.848051
5.455545	436.821015	5.853056
5.163935	433.944791	5.858061
5.056697	431.333375	5.863066
5.367736	430.617272	5.868070
5.281922	432.634405	5.873075
5.633232	432.772911	5.878080
5.535526	440.658088	5.883085
5.416935	424.872173	5.888090
5.440266	424.426873	5.893094
5.340002	445.940890	5.898099
5.450368	462.785465	5.903104
5.264005	463.352894	5.908109
5.386408	463.558333	5.913114
5.569293	463.571164	5.918118
5.824798	465.784850	5.923123
5.910282	465.493146	5.928128
5.584174	471.241211	5.933133
5.721528	453.109647	5.938138
5.912559	464.282481	5.943142
5.527351	475.003108	5.948147
5.780052	460.041434	5.953152
5.873713	471.181628	5.958157
5.700440	473.337822	5.963162
5.642993	460.193051	5.968166
5.488055	474.857974	5.973171
5.640736	464.199532	5.978176
5.652569	462.631058	5.983181
5.852631	466.673913	5.988186
5.625780	464.797515	5.993190
5.321059	471.395420	5.998195
5.847675	461.874449	6.003200
5.628355	477.843197	6.008205
5.642295	470.843947	6.013210
5.966281	481.849501	6.018214
5.810081	485.155081	6.023219
5.674952	479.878532	6.028224
5.682519	495.325500	6.033229
5.803590	498.027853	6.038234
6.016511	500.654157	6.043238
5.953867	500.018944	6.048243
6.073865	487.243397	6.053248
5.684705	480.449271	6.058253
5.969033	485.994551	6.063258
5.684131	486.062095	6.068262
5.834399	500.164085	6.073267
5.982199	493.703663	6.078272
5.803689	497.241321	6.083277
6.046138	494.935556	6.088282
5.599662	480.820153	6.093286
5.701137	500.744804	6.098291
5.968615	498.086942	6.103296
5.963998	497.621891	6.108301
6.041375	502.419032	6.113306
5.912759	475.283828	6.118310
6.000655	461.745273	6.123315
6.192150	465.020224	6.128320
5.879910	477.413247	6.133325
5.934159	463.217184	6.138330
5.828251	455.231061	6.143334
5.648854	468.105466	6.148339
5.895116	455.066584	6.153344
5.792775	462.940107	6.158349
5.823461	473.254303	6.163354
5.927509	463.221684	6.168358
5.768484	465.692998	6.173363
5.833053	466.075710	6.178368
5.861693	465.421269	6.183373
5.978498	465.156649	6.188378
5.854829	458.981726	6.193382
5.598140	471.939151	6.198387
5.731808	472.502724	6.203392
6.150588	464.899491	6.208397
6.140898	459.490935	6.213402
5.956804	461.896345	6.218406
5.646662	466.793919	6.223411
5.838080	459.473422	6.228416
5.862499	466.812395	6.233421
5.522833	460.808128	6.238426
5.672030	458.627090	6.243430
5.415932	473.566122	6.248435
5.715857	482.817306	6.253440
5.799709	488.195543	6.258445
6.054786	495.853548	6.263450
6.219702	502.310025	6.268454
6.097538	481.225223	6.273459
6.008881	466.605959	6.278464
5.561902	462.845993	6.283469
5.574605	470.030338	6.288474
5.817072	470.096069	6.293478
5.646498	480.952990	6.298483
6.216269	488.701545	6.303488
5.928530	494.825964	6.308493
5.712226	470.255228	6.313498
6.166897	462.788030	6.318502
5.766543	472.635389	6.323507
6.248035	460.022891	6.328512
5.796428	463.913578	6.333517
5.716822	471.073024	6.338522
5.748805	466.152340	6.343526
5.480838	475.413213	6.348531
5.558941	475.754720	6.353536
5.956512	483.818621	6.358541
5.974687	499.979592	6.363546
5.862170	490.816882	6.368550
5.703397	492.586318	6.373555
5.942336	492.402242	6.378560
5.967456	495.801476	6.383565
5.939969	483.305825	6.388570
6.011123	474.511738	6.393574
5.933413	484.553708	6.398579
5.692582	468.846847	6.403584
5.539748	479.204003	6.408589
5.758006	488.291994	6.413594
5.997352	490.527493	6.418598
5.674091	501.873839	6.423603
6.061624	494.131914	6.428608
5.980924	494.796323	6.433613
5.743039	487.255623	6.438618
5.893504	469.882512	6.443622
5.902096	477.542372	6.448627
5.937257	471.482866	6.453632
5.650607	470.843434	6.458637
5.622383	474.971569	6.463642
5.796448	491.065727	6.468646
5.812568	500.268520	6.473651
6.126022	488.700816	6.478656
5.962791	488.752200	6.483661
5.588245	485.076251	6.488666
5.807614	491.521751	6.493670
5.971553	490.184250	6.498675
5.920905	485.922820	6.503680
5.938010	494.431500	6.508685
5.903741	481.979393	6.513690
5.740860	465.033654	6.518694
5.653265	486.854921	6.523699
5.850303	486.847360	6.528704
5.646310	503.894183	6.533709
6.109723	507.963771	6.538714
6.024215	506.159214	6.543718
5.751726	499.410320	6.548723
6.052584	486.304181	6.553728
5.720234	484.882459	6.558733
5.750059	482.751629	6.563738
5.852276	493.718961	6.568742
5.778616	512.971026	6.573747
6.170877	503.823054	6.578752
5.715794	485.480957	6.583757
5.653788	490.275478	6.588762
5.918789	498.563343	6.593766
6.112302	510.292715	6.598771
5.949450	498.258738	6.603776
5.585311	481.852643	6.608781
5.750966	490.704265	6.613786
6.054534	497.954306	6.618790
5.812732	499.705203	6.623795
5.803143	475.438984	6.628800
5.854212	493.718480	6.633805
5.811749	490.163358	6.638810
5.907598	493.032760	6.643814
5.871330	504.552967	6.648819
6.088276	486.692735	6.653824
5.538635	494.755128	6.658829
5.676929	498.380820	6.663834
5.891648	503.078313	6.668838
6.075207	505.907967	6.673843
6.076406	501.906014	6.678848
5.833206	484.672526	6.683853
5.457605	481.477307	6.688858
5.945842	497.173171	6.693862
5.857333	500.076790	6.698867
5.898533	497.656890	6.703872
5.660683	502.694262	6.708877
5.737000	505.741023	6.713882
6.349402	503.094133	6.718886
5.687586	499.662769	6.723891
5.843104	480.869246	6.728896
5.640217	485.529493	6.733901
5.676908	503.211053	6.738906
6.118797	502.162260	6.743910
5.733740	509.775706	6.748915
5.670782	508.177461	6.753920
6.279317	503.235083	6.758925
5.994634	495.138194	6.763930
5.836557	488.818888	6.768934
5.785227	481.272716	6.773939
5.609907	467.665877	6.778944
5.945193	496.721574	6.783949
6.123088	498.220303	6.788954
6.142494	483.738055	6.793958
5.899003	478.136584	6.798963
5.710478	466.631725	6.803968
5.667796	473.961073	6.808973
5.658283	472.121764	6.813978
5.997294	476.986944	6.818982
5.549281	478.150087	6.823987
5.989155	478.074476	6.828992
5.935671	488.980521	6.833997
5.761947	484.466646	6.839002
6.031716	480.256547	6.844006
5.829456	483.646591	6.849011
5.684152	465.967989	6.854016
5.806033	473.838796	6.859021
5.910966	499.395053	6.864026
6.326551	483.045279	6.869030
5.519740	488.272368	6.874035
5.545147	483.563100	6.879040
6.041826	482.311492	6.884045
5.765590	488.914069	6.889050
6.086154	490.394548	6.894054
6.094017	481.732559	6.899059
5.835019	468.451795	6.904064
6.032967	474.419485	6.909069
5.555045	469.579513	6.914074
5.808428	469.572013	6.919078
5.588671	474.534367	6.924083
5.943778	482.189943	6.929088
6.090567	479.020370	6.934093
5.728507	478.169056	6.939098
5.825564	471.854654	6.944102
5.775241	490.919630	6.949107
5.886892	469.206833	6.954112
5.716232	480.833680	6.959117
5.833937	480.324245	6.964122
5.961958	484.329386	6.969126
5.797267	491.228046	6.974131
5.804574	479.570849	6.979136
6.044060	476.319859	6.984141
5.939860	483.651387	6.989146
6.166356	483.616366	6.994150
5.684831	474.163826	6.999155
5.786988	482.183414	7.004160
6.191054	481.207761	7.009165
5.614097	485.413558	7.014170
5.935836	479.517617	7.019174
5.803039	483.657117	7.024179
5.685974	484.102994	7.029184
5.848067	490.039521	7.034189
5.589306	481.675238	7.039194
5.891297	475.486298	7.044198
5.592029	497.481665	7.049203
5.749833	499.844096	7.054208
5.762666	503.156275	7.059213
5.392227	510.204866	7.064218
5.943418	519.723738	7.069222
6.027256	506.579356	7.074227
6.166838	514.329265	7.079232
5.963359	511.254172	7.084237
5.957637	515.340814	7.089242
6.050969	502.839288	7.094246
5.675234	501.124227	7.099251
5.712909	485.181115	7.104256
5.861893	510.820579	7.109261
5.784842	515.067881	7.114266
5.812348	510.375917	7.119270
5.925567	509.629460	7.124275
5.757192	515.076716	7.129280
5.995419	510.374001	7.134285
5.803629	514.528388	7.139290
6.357640	492.599009	7.144294
5.975168	491.018544	7.149299
5.960407	491.535319	7.154304
5.829281	474.915412	7.159309
5.607655	484.308133	7.164314
5.889567	479.603732	7.169318
5.738858	477.308681	7.174323
5.723080	477.447573	7.179328
5.928612	480.557030	7.184333
5.852620	475.845776	7.189338
5.761569	473.328263	7.194342
5.720603	484.771490	7.199347
5.695975	484.890535	7.204352
6.394625	498.326932	7.209357
6.007172	495.980336	7.214362
5.722360	482.002972	7.219366
5.657848	485.318359	7.224371
5.367391	475.098466	7.229376
5.724403	493.936900	7.234381
5.967950	509.791897	7.239386
6.172691	506.906738	7.244390
5.814471	487.925419	7.249395
5.519218	486.571262	7.254400
5.960033	503.934860	7.259405
5.835781	514.951965	7.264410
6.012382	511.696857	7.269414
5.890713	518.638242	7.274419
5.835478	502.620886	7.279424
5.843433	501.812702	7.284429
5.814184	506.054470	7.289434
5.708321	503.917351	7.294438
6.055712	519.107223	7.299443
6.011477	512.162851	7.304448
6.042199	481.974231	7.309453
5.457779	481.821448	7.314458
5.871282	491.006019	7.319462
5.833435	497.724293	7.324467
6.147102	500.383868	7.329472
5.867353	497.759909	7.334477
5.631653	490.585354	7.339482
5.693993	486.991801	7.344486
5.333349	501.422990	7.349491
5.729308	509.371447	7.354496
5.908435	509.482372	7.359501
5.617430	529.029841	7.364506
6.124079	504.999489	7.369510
5.852827	521.315255	7.374515
6.023316	511.493898	7.379520
5.904720	518.736367	7.384525
6.027658	511.896766	7.389530
6.099440	506.146402	7.394534
5.821838	505.386789	7.399539
6.192961	497.729755	7.404544
5.720902	487.842837	7.409549
5.422947	483.709194	7.414554
6.140283	489.135365	7.419558
5.995129	502.884647	7.424563
5.824902	488.594937	7.429568
5.735625	478.591889	7.434573
5.529181	488.323157	7.439578
5.779314	499.314785	7.444582
5.887696	515.967663	7.449587
6.028335	514.123660	7.454592
6.002451	517.264659	7.459597
5.928835	503.997525	7.464602
5.498629	482.016724	7.469606
5.751974	510.523352	7.474611
5.838059	514.438649	7.479616
5.910939	510.702566	7.484621
5.579499	514.935574	7.489626
6.243936	506.668906	7.494630
5.912404	511.840644	7.499635
5.934659	518.141938	7.504640
6.020972	504.285046	7.509645
5.789008	495.767357	7.514650
5.838999	486.263278	7.519654
5.473897	494.658131	7.524659
5.642318	505.875082	7.529664
6.080281	508.536119	7.534669
5.912427	519.747879	7.539674
6.107906	512.350424	7.544678
5.882280	503.820930	7.549683
5.404480	502.314918	7.554688
5.703415	506.509949	7.559693
5.736943	524.029273	7.564698
5.849104	513.853017	7.569702
5.789468	511.219712	7.574707
5.795883	516.101492	7.579712
5.804540	517.267207	7.584717
5.666039	518.058176	7.589722
5.998712	513.022080	7.594726
5.628672	528.897993	7.599731
5.919529	530.784127	7.604736
6.032372	514.940241	7.609741
5.861148	521.506833	7.614746
6.150884	516.139933	7.619750
6.043946	528.898530	7.624755
6.035471	519.890963	7.629760
6.363775	506.928157	7.634765
5.970283	503.499311	7.639770
5.624121	495.346975	7.644774
5.458953	493.536937	7.649779
5.534115	490.979819	7.654784
6.000672	505.951488	7.659789
5.828094	516.486948	7.664794
6.014827	510.670132	7.669798
5.981596	520.465829	7.674803
5.941226	513.420583	7.679808
5.888457	494.466520	7.684813
5.772826	488.902714	7.689818
5.773781	485.591300	7.694822
5.332510	509.473471	7.699827
5.669491	503.665470	7.704832
5.829510	507.468805	7.709837
5.609434	515.151674	7.714842
6.152399	506.919187	7.719846
5.958566	513.049208	7.724851
5.681227	517.005622	7.729856
5.550872	513.128601	7.734861
5.710910	510.828462	7.739866
5.963741	519.011504	7.744870
5.940278	526.636532	7.749875
5.893564	518.492313	7.754880
5.892698	509.306011	7.759885
5.693263	516.570027	7.764890
5.791983	508.853823	7.769894
5.805380	520.264514	7.774899
5.776964	525.481565	7.779904
6.189325	515.135436	7.784909
5.857068	518.687852	7.789914
6.114393	520.541642	7.794918
5.778416	514.542663	7.799923
5.229991	514.849097	7.804928
5.544275	511.934784	7.809933
5.567373	523.195002	7.814938
5.643992	508.037641	7.819942
5.493635	519.279659	7.824947
5.842548	516.176221	7.829952
6.178530	525.311568	7.834957
5.780081	513.726727	7.839962
6.307489	516.437406	7.844966
5.945695	519.658186	7.849971
6.072681	510.362951	7.854976
6.156421	515.911892	7.859981
5.778534	524.971450	7.864986
6.128718	517.385348	7.869990
5.896644	510.951686	7.874995
5.619426	523.359577	7.880000
5.776393	515.640354	7.885005
5.631018	520.290318	7.890010
5.849928	517.519427	7.895014
5.672116	517.760668	7.900019
5.834453	516.293498	7.905024
5.826298	512.715042	7.910029
6.003070	529.504715	7.915034
5.987577	514.664064	7.920038
6.133527	507.490262	7.925043
5.917309	525.952776	7.930048
5.831630	510.659451	7.935053
5.969723	523.543096	7.940058
6.199811	521.742419	7.945062
6.119897	522.334089	7.950067
6.142423	518.472843	7.955072
6.132533	510.489667	7.960077
5.720517	502.834979	7.965082
5.811639	488.244686	7.970086
5.994892	502.888671	7.975091
5.413252	493.248248	7.980096
5.982733	499.517013	7.985101
5.700857	511.146675	7.990106
5.910372	511.418814	7.995110
5.811951	517.989059	8.000115
5.717833	520.329390	8.005133
5.934558	519.234978	8.010150
5.871151	519.363288	8.015168
6.053008	517.837524	8.020186
5.775959	525.927936	8.025203
5.838520	521.768008	8.030221
6.108647	513.753021	8.035238
5.968393	520.286695	8.040256
6.039667	498.779936	8.045274
5.931062	484.788463	8.050291
5.656110	480.451990	8.055309
5.924689	486.581052	8.060326
5.604555	511.794083	8.065344
5.719494	518.850328	8.070362
6.072855	521.224440	8.075379
5.834071	518.537048	8.080397
6.186901	514.380718	8.085414
6.151847	511.416502	8.090432
6.007790	505.532330	8.095450
5.881339	501.676717	8.100467
5.757666	500.629112	8.105485
6.179003	505.893546	8.110502
5.921453	518.562846	8.115520
6.212556	503.642292	8.120538
5.980452	492.110968	8.125555
5.564126	502.327289	8.130573
6.179604	502.706817	8.135590
5.921391	509.685383	8.140608
6.269563	517.369973	8.145626
5.657341	512.486695	8.150643
6.030558	508.375707	8.155661
6.447761	513.845017	8.160678
5.485223	501.391108	8.165696
5.935083	500.751571	8.170714
6.168827	515.651105	8.175731
5.850992	517.286509	8.180749
6.157969	509.887352	8.185766
5.661266	517.824827	8.190784
5.651624	521.645844	8.195802
5.918958	513.714962	8.200819
5.951583	517.280324	8.205837
5.845182	519.085470	8.210854
5.787982	520.333682	8.215872
5.942221	510.262886	8.220890
5.905383	518.612846	8.225907
5.652771	521.889196	8.230925
6.375625	521.593439	8.235942
5.942527	533.620543	8.240960
6.022726	519.322994	8.245978
5.838162	535.266373	8.250995
5.790728	532.242893	8.256013
6.157356	533.651431	8.261030
6.204664	538.250870	8.266048
6.246074	537.117824	8.271066
6.307946	533.365305	8.276083
5.976723	552.095555	8.281101
6.116712	542.247421	8.286118
6.079434	540.102394	8.291136
5.978838	541.084706	8.296154
6.236771	539.743670	8.301171
6.290458	539.144704	8.306189
6.416980	548.744193	8.311206
5.815718	542.243974	8.316224
6.105222	538.675935	8.321242
6.359657	542.954985	8.326259
6.242799	549.440326	8.331277
6.263284	553.539089	8.336294
6.298072	541.708950	8.341312
6.064397	541.167510	8.346330
6.188644	544.327267	8.351347
6.120220	557.798637	8.356365
6.684712	542.303842	8.361382
6.088819	550.630778	8.366400
6.312316	552.670228	8.371418
6.442067	547.490146	8.376435
6.228628	556.474600	8.381453
6.236425	541.206815	8.386470
6.195864	535.743037	8.391488
6.343623	536.447938	8.396506
6.325683	524.775116	8.401523
6.240571	521.112920	8.406541
6.188229	517.553160	8.411558
6.084229	525.287680	8.416576
6.027634	534.550568	8.421594
6.445111	535.777314	8.426611
6.208362	547.228688	8.431629
6.403160	534.387767	8.436646
6.347842	536.930382	8.441664
6.316247	546.905434	8.446682
6.495109	535.885078	8.451699
6.287759	546.485607	8.456717
6.503777	533.704749	8.461734
6.303962	545.328623	8.466752
5.950605	545.609355	8.471770
6.405869	549.223458	8.476787
6.386302	546.394935	8.481805
5.972561	529.730098	8.486822
6.559650	542.189575	8.491840
6.123400	541.769684	8.496858
6.377313	533.444143	8.501875
6.180473	545.663564	8.506893
6.176061	531.353514	8.511910
6.613946	539.931763	8.516928
6.008516	538.469481	8.521946
6.458090	537.309428	8.526963
6.316934	541.380679	8.531981
6.117719	534.873262	8.536998
5.965204	542.441435	8.542016
6.363404	542.897610	8.547034
6.364059	545.787202	8.552051
6.088513	553.512298	8.557069
6.407496	562.367636	8.562087
6.725039	577.233011	8.567104
6.128153	569.202941	8.572122
6.491008	570.268772	8.577139
6.162238	582.412996	8.582157
6.490816	572.265425	8.587175
6.515220	574.254529	8.592192
6.598792	579.084454	8.597210
6.709083	576.280420	8.602227
6.464215	566.226636	8.607245
6.875937	560.866416	8.612263
6.431227	557.636394	8.617280
6.330371	559.650034	8.622298
6.512823	556.586197	8.627315
6.348973	570.484484	8.632333
6.664618	571.322141	8.637351
6.770739	573.562450	8.642368
6.069569	568.538275	8.647386
6.232186	575.434631	8.652403
6.521662	572.547651	8.657421
6.718350	568.643933	8.662439
6.657102	589.102282	8.667456
6.743243	585.255207	8.672474
6.691295	570.254792	8.677491
6.436165	565.543048	8.682509
6.749414	573.838924	8.687527
6.781164	580.006570	8.692544
6.715603	570.002958	8.697562
6.707084	557.769909	8.702579
6.394628	547.746396	8.707597
6.597351	559.893794	8.712615
6.702441	557.316168	8.717632
6.605509	564.547871	8.722650
6.767089	556.748988	8.727667
6.204978	545.463556	8.732685
6.417053	560.345262	8.737703
6.828976	577.961206	8.742720
6.583671	576.223507	8.747738
6.619710	573.341802	8.752755
6.769696	574.498901	8.757773
6.873805	568.305246	8.762791
7.006898	568.588053	8.767808
6.575602	566.082534	8.772826
6.751364	549.553181	8.777843
6.555341	549.050982	8.782861
6.463051	553.394320	8.787879
6.675712	567.069097	8.792896
6.642093	566.395995	8.797914
6.690242	572.911152	8.802931
6.385149	578.203059	8.807949
6.901582	582.266024	8.812967
7.038748	572.867556	8.817984
6.706971	573.938064	8.823002
6.992860	577.762706	8.828019
6.629763	578.767342	8.833037
6.844429	576.327871	8.838055
7.018904	578.652830	8.843072
6.784199	567.232880	8.848090
6.634574	560.536291	8.853107
6.533620	556.957592	8.858125
6.633239	574.151027	8.863143
6.746972	579.527626	8.868160
6.331318	569.269729	8.873178
6.547563	566.989120	8.878195
6.652842	581.347070	8.883213
6.468592	576.083070	8.888231
6.532790	578.693619	8.893248
6.344474	585.651419	8.898266
6.611459	581.758517	8.903283
6.662070	599.852810	8.908301
6.540022	614.521827	8.913319
7.166090	605.876334	8.918336
7.031592	593.801253	8.923354
7.030751	615.541123	8.928371
7.050888	616.023270	8.933389
6.710966	599.453716	8.938407
6.971260	594.218784	8.943424
6.863673	612.172438	8.948442
6.993128	591.495529	8.953459
7.266664	585.971659	8.958477
6.808417	597.508876	8.963495
6.806089	573.025118	8.968512
6.736536	573.855383	8.973530
6.604607	596.158708	8.978547
6.617113	595.126282	8.983565
6.638322	611.523529	8.988583
6.937436	612.213164	8.993600
6.647671	610.545590	8.998618
7.077968	605.745360	9.003635
6.982412	608.020086	9.008653
6.474227	619.955159	9.013671
6.895745	608.044232	9.018688
6.650437	617.154239	9.023706
6.638225	606.051947	9.028723
6.852459	606.181413	9.033741
6.682790	616.139671	9.038759
6.993543	625.667235	9.043776
7.325669	634.385529	9.048794
7.149795	629.824709	9.053811
7.175076	627.614519	9.058829
7.503963	611.580655	9.063847
7.461528	595.880162	9.068864
6.863608	600.574734	9.073882
7.095916	620.841040	9.078899
7.088088	605.966146	9.083917
6.969391	607.902344	9.088935
7.077103	606.135726	9.093952
6.774721	620.074959	9.098970
6.698206	595.095458	9.103987
7.157713	598.980372	9.109005
6.639331	610.419291	9.114023
7.217710	605.141532	9.119040
7.086333	626.607972	9.124058
7.317501	628.828412	9.129075
7.029640	615.982065	9.134093
6.868629	618.880575	9.139111
7.067483	628.280206	9.144128
7.103055	644.285134	9.149146
7.657120	626.734318	9.154163
6.962241	620.465241	9.159181
7.075203	627.330071	9.164199
7.608462	628.226731	9.169216
7.304796	616.363212	9.174234
7.221127	608.601190	9.179251
7.118558	608.425110	9.184269
6.906698	607.360384	9.189287
7.260506	605.551425	9.194304
7.217222	606.446628	9.199322
7.409017	615.698431	9.204339
7.263455	613.049937	9.209357
7.006968	607.522525	9.214375
7.053350	602.044946	9.219392
6.763820	607.993607	9.224410
7.274395	633.372448	9.229427
7.242283	642.852866	9.234445
7.396364	644.185440	9.239463
7.826235	626.480577	9.244480
7.332706	637.733359	9.249498
7.142926	615.332462	9.254515
7.185829	593.119774	9.259533
7.203207	610.539001	9.264551
7.215032	615.002721	9.269568
7.132867	623.139899	9.274586
7.584104	632.859956	9.279603
7.351762	630.615879	9.284621
7.243742	633.595283	9.289639
7.685825	619.870878	9.294656
7.380396	619.607775	9.299674
7.099243	612.543902	9.304691
7.243031	614.164140	9.309709
7.151558	632.258827	9.314727
7.236973	640.036694	9.319744
7.408599	639.344726	9.324762
7.222681	642.666170	9.329779
7.406205	645.634102	9.334797
7.351138	644.925670	9.339815
7.155132	640.888641	9.344832
7.395282	643.532415	9.349850
7.512554	632.703431	9.354867
7.440729	631.553862	9.359885
7.276802	648.120101	9.364903
7.679929	633.779117	9.369920
7.427937	634.835066	9.374938
7.207734	644.497915	9.379955
7.233588	636.634528	9.384973
7.180803	634.064381	9.389991
7.344324	638.635099	9.395008
7.310171	636.219714	9.400026
7.419317	649.502698	9.405043
7.560576	639.645338	9.410061
6.940598	633.749725	9.415079
7.258105	648.671168	9.420096
7.590743	633.970745	9.425114
7.385559	638.417589	9.430131
7.280079	642.014659	9.435149
7.719539	642.948272	9.440167
8.027553	633.185283	9.445184
7.673844	639.735881	9.450202
7.568850	648.656118	9.455219
7.834772	651.799865	9.460237
7.371840	649.703810	9.465255
7.533072	635.417363	9.470272
7.612043	640.522323	9.475290
7.302406	647.591815	9.480307
7.675355	638.790437	9.485325
7.646362	635.253262	9.490343
7.919049	629.422590	9.495360
8.053607	640.563608	9.500378
7.652976	636.560691	9.505395
7.766124	630.705311	9.510413
7.695933	637.284039	9.515431
7.864860	641.798561	9.520448
7.725467	645.430463	9.525466
7.793444	640.560596	9.530483
7.740600	637.601657	9.535501
7.898459	633.529867	9.540519
7.450752	627.978744	9.545536
7.530931	630.933836	9.550554
7.337906	635.456312	9.555571
7.406848	639.490113	9.560589
7.534689	637.524732	9.565607
7.496748	637.340234	9.570624
7.372602	642.109545	9.575642
7.457459	638.295930	9.580659
7.690966	640.481149	9.585677
7.569066	645.355482	9.590695
7.703270	636.937781	9.595712
7.536318	637.357754	9.600730
7.569217	639.551130	9.605747
7.761529	638.612092	9.610765
7.308654	644.720510	9.615783
7.717661	654.000896	9.620800
7.898876	658.235298	9.625818
7.708952	666.669385	9.630835
8.007543	669.270934	9.635853
7.860070	663.456741	9.640871
7.757393	647.497504	9.645888
7.831956	655.932357	9.650906
7.570176	654.596701	9.655923
8.072370	653.927450	9.660941
7.537218	667.009899	9.665959
7.810110	675.221277	9.670976
7.736619	669.577300	9.675994
7.498892	675.491545	9.681011
7.793092	668.959016	9.686029
7.538211	670.565729	9.691047
7.779339	675.556225	9.696064
7.686055	677.895336	9.701082
7.710556	661.558839	9.706099
7.858990	668.258998	9.711117
7.456000	673.890674	9.716135
7.767955	681.120006	9.721152
7.957355	669.763725	9.726170
7.755817	660.393230	9.731187
8.037773	671.614124	9.736205
8.082198	674.683674	9.741223
8.125948	671.760331	9.746240
7.986374	666.895430	9.751258
7.945408	677.511851	9.756275
8.066547	670.073854	9.761293
8.004498	667.825837	9.766311
7.822593	657.251845	9.771328
7.925756	663.336872	9.776346
7.930595	666.904105	9.781363
8.202073	657.642808	9.786381
7.746060	674.084643	9.791399
7.664277	670.799738	9.796416
7.862334	662.591408	9.801434
7.850956	672.710318	9.806451
8.037889	676.413570	9.811469
8.418831	694.093810	9.816487
7.855298	684.955431	9.821504
8.069639	667.383068	9.826522
7.972449	678.830075	9.831539
8.154782	666.540898	9.836557
8.325401	669.288767	9.841575
8.335607	675.089613	9.846592
8.260325	659.402061	9.851610
8.014681	677.311296	9.856627
7.716494	658.420475	9.861645
7.807439	670.419340	9.866663
7.906560	688.367756	9.871680
8.235023	690.998420	9.876698
8.310796	698.397572	9.881715
8.407715	685.238712	9.886733
8.190863	666.220879	9.891751
8.067432	678.357323	9.896768
8.228278	668.643922	9.901786
8.305982	662.273034	9.906803
8.527593	657.925892	9.911821
8.066013	669.725473	9.916839
8.155883	654.968121	9.921856
8.319878	663.765486	9.926874
8.036815	664.376661	9.931891
8.179990	663.895750	9.936909
8.160302	666.831730	9.941927
8.143010	672.356564	9.946944
8.695236	665.091474	9.951962
8.079306	666.769465	9.956979
7.891829	668.306586	9.961997
8.398634	666.234292	9.967015
8.108609	666.071772	9.972032
8.207568	665.609288	9.977050
7.820394	669.282536	9.982067
8.329224	689.974206	9.987085
8.283284	697.602681	9.992103
8.581237	702.129750	9.997120
8.614688	692.006468	10.002138
8.096028	678.662882	10.007155
8.050164	683.944559	10.012173
8.285233	686.474833	10.017191
8.491015	690.483180	10.022208
8.848762	702.167167	10.027226
8.255566	680.721251	10.032243
8.056705	671.758592	10.037261
8.135682	680.362479	10.042279
8.399457	696.009537	10.047296
8.621180	705.207147	10.052314
8.437454	705.524403	10.057331
8.331196	689.728576	10.062349
8.620226	707.297372	10.067367
8.197087	695.933855	10.072384
8.431576	688.817995	10.077402
8.652011	687.369189	10.082419
8.568627	684.117610	10.087437
8.188643	675.939653	10.092455
8.377885	694.961847	10.097472
8.750504	695.274252	10.102490
8.339686	669.229821	10.107507
8.010501	683.909911	10.112525
8.462600	695.037264	10.117543
8.437478	689.622051	10.122560
8.581061	700.802164	10.127578
8.710109	701.316109	10.132595
8.569916	693.401507	10.137613
8.608219	701.600988	10.142631
8.535634	704.949377	10.147648
8.425420	694.987504	10.152666
8.210508	691.367973	10.157683
8.713891	693.524937	10.162701
8.928216	697.028036	10.167719
8.852800	707.058949	10.172736
8.969511	684.962350	10.177754
8.257811	680.889099	10.182771
8.479890	662.597396	10.187789
8.437066	673.159407	10.192807
8.299246	679.829727	10.197824
8.608844	682.658843	10.202842
8.375666	697.624989	10.207859
8.567390	694.388465	10.212877
8.461967	691.680184	10.217895
8.025465	701.840042	10.222912
8.640137	698.351079	10.227930
8.234898	703.719607	10.232947
8.451396	700.262002	10.237965
8.794951	699.482576	10.242983
8.365370	692.936798	10.248000
8.487770	687.416219	10.253018
8.481395	702.870081	10.258035
8.665985	712.835297	10.263053
8.918012	723.958538	10.268071
8.769317	713.936391	10.273088
8.950254	702.487310	10.278106
8.690485	708.785550	10.283123
8.417181	698.597330	10.288141
8.810443	707.180291	10.293159
8.753718	725.887827	10.298176
8.940099	729.153276	10.303194
8.808021	715.958723	10.308211
8.810561	722.689708	10.313229
8.878060	708.659482	10.318247
8.272958	713.545788	10.323264
8.703824	708.687275	10.328282
8.722270	724.327965	10.333299
8.611594	722.401595	10.338317
8.994638	713.775932	10.343335
8.437388	730.674826	10.348352
9.085992	719.151990	10.353370
9.181744	715.575682	10.358387
8.648235	726.642063	10.363405
8.838794	724.693073	10.368423
8.906806	727.266804	10.373440
8.637503	723.454127	10.378458
8.777404	720.280285	10.383475
8.778193	723.924367	10.388493
9.264783	724.576038	10.393511
9.002609	728.140078	10.398528
9.167479	721.101837	10.403546
9.096594	732.240855	10.408563
8.904673	723.924236	10.413581
9.151324	714.489188	10.418599
9.205885	735.848492	10.423616
9.376526	723.415364	10.428634
9.011443	715.301052	10.433651
9.070934	701.124842	10.438669
8.964285	690.066339	10.443687
8.718037	702.031403	10.448704
9.129512	714.914551	10.453722
9.077554	708.538305	10.458739
8.756133	705.233754	10.463757
8.829407	696.645613	10.468775
8.725744	717.102186	10.473792
9.029020	717.233274	10.478810
9.188733	720.400787	10.483827
9.187921	730.615115	10.488845
9.248144	723.462991	10.493863
9.192878	719.547241	10.498880
9.159385	716.610084	10.503898
9.491513	728.998975	10.508915
9.169149	717.394422	10.513933
9.249158	693.179784	10.518951
8.761893	700.517288	10.523968
8.957396	713.084521	10.528986
9.163960	709.849378	10.534003
8.901320	724.006011	10.539021
8.829289	714.077671	10.544039
8.893749	726.020436	10.549056
9.175380	713.657933	10.554074
9.738882	718.337443	10.559091
8.970743	727.852358	10.564109
8.849455	719.359928	10.569127
8.921838	723.923197	10.574144
9.181121	724.371141	10.579162
9.324543	717.776813	10.584179
9.333523	717.621659	10.589197
9.630521	718.655381	10.594215
9.584232	731.436568	10.599232
9.196837	724.915098	10.604250
9.293285	724.908943	10.609267
8.968443	726.627204	10.614285
8.951020	717.839711	10.619303
9.038919	726.321109	10.624320
8.995089	729.157764	10.629338
9.072383	711.768302	10.634355
9.081240	728.224299	10.639373
8.970955	726.023509	10.644391
8.959039	734.406469	10.649408
9.316936	751.125416	10.654426
9.358965	758.144814	10.659443
9.368926	759.213869	10.664461
9.878327	750.663447	10.669479
9.739196	766.333172	10.674496
9.694202	746.534819	10.679514
9.692932	733.364787	10.684531
9.181225	726.066770	10.689549
9.339350	718.883020	10.694567
9.277115	709.420000	10.699584
9.587077	711.541818	10.704602
9.599869	710.713725	10.709619
9.294382	720.579557	10.714637
9.311033	716.774930	10.719655
9.424297	722.068012	10.724672
9.430057	721.847262	10.729690
9.733051	719.536255	10.734707
9.389685	721.573165	10.739725
9.498395	720.688973	10.744743
9.449529	719.834265	10.749760
9.363699	723.317892	10.754778
9.442156	738.292311	10.759795
9.647092	747.252216	10.764813
9.523548	737.074451	10.769831
9.765237	742.812073	10.774848
9.684085	743.514270	10.779866
9.799262	731.396442	10.784883
9.371104	734.013201	10.789901
9.355550	721.116058	10.794919
9.514453	732.049222	10.799936
9.651805	743.582198	10.804954
9.728156	751.063842	10.809971
9.687724	744.126926	10.814989
9.365319	732.744471	10.820007
9.645548	739.250474	10.825024
9.703332	743.768239	10.830042
9.926763	754.525728	10.835059
9.735259	736.965149	10.840077
9.324960	727.832025	10.845095
9.709220	737.618620	10.850112
9.537644	753.651892	10.855130
9.789329	749.985548	10.860147
10.110111	746.399796	10.865165
9.806536	740.450279	10.870183
9.421420	727.445535	10.875200
9.810394	748.589684	10.880218
9.910580	754.241759	10.885235
9.531613	732.239308	10.890253
9.358350	736.157482	10.895271
9.688251	755.909707	10.900288
9.592156	755.170753	10.905306
10.005615	752.453077	10.910323
9.930393	756.447064	10.915341
10.119242	748.800142	10.920359
9.923563	761.644322	10.925376
9.775645	757.459676	10.930394
9.796191	765.294085	10.935411
9.763776	764.230496	10.940429
9.875194	769.770407	10.945447
9.791015	752.891349	10.950464
9.902981	763.818023	10.955482
9.604888	755.144890	10.960499
9.771425	763.442677	10.965517
9.794638	749.376434	10.970535
9.974828	754.369153	10.975552
9.840165	760.240223	10.980570
10.041558	756.708837	10.985587
9.876508	759.664822	10.990605
10.044869	751.483395	10.995623
9.814533	754.965422	11.000640
9.444910	760.904646	11.005658
9.815399	764.448969	11.010675
9.669631	754.136309	11.015693
9.530821	758.795699	11.020711
9.858337	755.688660	11.025728
9.608597	775.655082	11.030746
10.358472	763.627481	11.035763
9.870817	782.234383	11.040781
10.120983	796.818150	11.045799
10.421698	784.726695	11.050816
9.971892	769.269591	11.055834
10.266212	763.359226	11.060851
9.919834	768.840860	11.065869
10.050625	754.116111	11.070887
10.465795	751.996068	11.075904
10.354900	756.459346	11.080922
10.430159	745.183966	11.085939
9.949856	751.375978	11.090957
9.998562	751.149410	11.095975
10.291533	755.893615	11.100992
9.989344	752.469265	11.106010
10.368452	745.347291	11.111027
10.245953	752.880494	11.116045
9.873428	742.962529	11.121063
10.113385	746.383860	11.126080
9.885237	761.380727	11.131098
10.057394	747.448503	11.136115
10.401775	759.454463	11.141133
10.036121	757.146391	11.146151
10.449933	747.515325	11.151168
9.978386	758.142733	11.156186
10.323441	752.702242	11.161203
10.095332	767.640753	11.166221
10.075753	782.210827	11.171239
10.310514	776.760410	11.176256
10.342722	781.597214	11.181274
10.561102	776.727150	11.186291
10.551115	787.927194	11.191309
9.993858	774.371834	11.196327
10.374147	766.735974	11.201344
10.078578	779.433913	11.206362
10.464385	782.892850	11.211379
10.319500	774.270751	11.216397
10.373295	780.685575	11.221415
10.216153	780.909086	11.226432
10.183059	775.770402	11.231450
10.333890	781.233543	11.236467
9.977912	795.840131	11.241485
10.055063	786.002816	11.246503
10.426908	784.623647	11.251520
10.107792	792.014297	11.256538
10.316206	770.350072	11.261555
10.134221	783.655206	11.266573
10.388595	789.631846	11.271591
10.315281	768.409381	11.276608
10.286959	799.735584	11.281626
10.723126	802.162284	11.286643
10.530808	806.883671	11.291661
10.285610	822.357439	11.296679
10.790244	810.030138	11.301696
10.781516	809.595483	11.306714
10.732537	794.239111	11.311731
10.787647	784.149682	11.316749
10.632827	793.291877	11.321767
10.839897	776.057044	11.326784
11.045563	762.704688	11.331802
10.802659	775.498821	11.336819
10.483312	776.382579	11.341837
10.365600	770.284642	11.346855
10.809748	767.316466	11.351872
10.543190	781.505978	11.356890
10.723611	774.827869	11.361907
10.981315	778.948108	11.366925
11.072449	779.978952	11.371943
11.067930	773.007649	11.376960
10.813601	781.264879	11.381978
10.643724	770.482858	11.386995
10.618571	767.664762	11.392013
10.610348	778.425222	11.397031
10.530875	771.638813	11.402048
10.498465	787.151087	11.407066
10.328485	771.104437	11.412083
10.366141	764.815898	11.417101
10.409122	783.946903	11.422119
10.521315	779.222806	11.427136
10.268472	778.532389	11.432154
10.536704	800.668031	11.437171
10.770034	804.243984	11.442189
10.730725	819.524897	11.447207
10.718600	814.350163	11.452224
10.749506	807.286195	11.457242
10.724225	813.593060	11.462259
10.746523	809.524633	11.467277
10.731082	816.708939	11.472295
10.891299	811.780182	11.477312
10.861246	816.386485	11.482330
10.715989	817.417722	11.487347
11.053398	815.591472	11.492365
11.123567	817.608668	11.497383
11.253390	806.903743	11.502400
11.173121	806.265499	11.507418
11.167896	812.165385	11.512435
10.927287	805.215566	11.517453
10.975220	816.367386	11.522471
10.777420	805.792770	11.527488
10.736522	822.046205	11.532506
10.797831	823.773877	11.537523
11.125143	814.920601	11.542541
10.802354	819.743164	11.547559
11.319064	810.967232	11.552576
11.099651	812.089547	11.557594
10.561092	818.518434	11.562611
10.934256	815.302481	11.567629
10.651976	816.952706	11.572647
11.024879	814.451820	11.577664
10.846727	812.539247	11.582682
10.636739	815.168971	11.587699
10.770995	805.880173	11.592717
10.895244	819.088479	11.597735
11.268153	836.511698	11.602752
11.549441	827.225552	11.607770
11.343187	811.440023	11.612787
11.370982	816.265168	11.617805
11.468024	804.836764	11.622823
11.229729	803.469856	11.627840
11.147153	813.344767	11.632858
11.077286	807.311435	11.637875
11.408496	810.731379	11.642893
11.002479	801.323441	11.647911
11.464204	799.633312	11.652928
11.115895	807.240269	11.657946
11.242966	810.591802	11.662963
11.094638	815.955799	11.667981
10.921009	812.771656	11.672999
10.765951	809.836857	11.678016
10.828943	818.263673	11.683034
10.953657	833.479017	11.688051
11.025087	837.093936	11.693069
11.455092	848.063272	11.698087
11.513022	840.717020	11.703104
11.398632	846.170086	11.708122
11.369371	848.619683	11.713139
11.561877	835.433188	11.718157
11.384078	843.668653	11.723175
11.688956	847.120018	11.728192
11.719533	841.512117	11.733210
11.663326	850.023794	11.738227
11.635034	824.054639	11.743245
11.662772	824.979743	11.748263
11.188223	806.183916	11.753280
11.207311	817.662687	11.758298
11.028286	821.220092	11.763315
11.308809	831.431491	11.768333
11.071811	841.974239	11.773351
11.290293	831.529988	11.778368
11.492808	847.032038	11.783386
11.449338	849.961158	11.788403
11.466161	837.602954	11.793421
11.148442	844.310848	11.798439
11.654832	845.272482	11.803456
11.549349	844.563909	11.808474
11.679925	843.722938	11.813491
12.095106	842.548177	11.818509
11.472397	846.825639	11.823527
11.361105	833.070667	11.828544
11.744412	839.844960	11.833562
11.837901	831.406623	11.838579
11.579542	833.968276	11.843597
12.012781	833.500437	11.848615
11.539952	828.202362	11.853632
11.480745	839.825264	11.858650
11.531227	842.170360	11.863667
11.881670	837.502525	11.868685
11.933537	849.549614	11.873703
11.682994	838.354577	11.878720
11.808163	831.990733	11.883738
11.520792	837.047756	11.888755
12.036432	836.435223	11.893773
11.889989	835.753790	11.898791
11.861870	841.257742	11.903808
11.971089	840.880254	11.908826
11.913784	837.023363	11.913843
12.186688	831.671525	11.918861
11.673687	829.990138	11.923879
11.616497	812.563152	11.928896
11.992091	818.903459	11.933914
11.950034	829.259682	11.938931
11.775305	814.504572	11.943949
11.704178	814.685528	11.948967
11.779233	826.524082	11.953984
11.980404	836.250069	11.959002
11.758527	848.599236	11.964019
12.278772	842.444753	11.969037
11.700558	840.221686	11.974055
12.025449	826.745753	11.979072
11.846900	839.307199	11.984090
11.787671	856.066066	11.989107
12.095468	827.986234	11.994125
11.777949	842.521562	11.999143
12.038890	857.847562	12.004160
12.159047	843.130488	12.009178
11.452373	842.584738	12.014195
12.180652	848.300836	12.019213
12.104325	849.025168	12.024231
12.104953	851.956153	12.029248
11.990794	845.735082	12.034266
11.745197	849.849653	12.039283
11.962884	847.467307	12.044301
11.866301	848.105142	12.049319
11.977148	852.915983	12.054336
12.055313	834.050038	12.059354
11.722001	848.753207	12.064371
11.984020	841.553706	12.069389
11.890863	848.163775	12.074407
11.602449	848.102935	12.079424
12.007298	851.898541	12.084442
12.221824	871.371021	12.089459
12.233653	878.380211	12.094477
12.364354	877.030552	12.099495
12.014430	869.062051	12.104512
12.237349	876.613809	12.109530
11.704709	881.245324	12.114547
11.708079	871.730425	12.119565
11.751662	873.205765	12.124583
12.005292	879.356152	12.129600
12.214747	860.902354	12.134618
12.136071	876.507290	12.139635
12.433749	868.385223	12.144653
12.482420	865.980028	12.149671
12.511323	878.535368	12.154688
12.623597	874.965543	12.159706
12.117664	870.705803	12.164723
12.155116	869.033428	12.169741
12.206094	868.075024	12.174759
12.129357	878.351594	12.179776
12.366384	868.196325	12.184794
11.806152	888.002431	12.189811
12.472559	892.739780	12.194829
12.758958	895.807667	12.199847
12.716187	904.852096	12.204864
12.945503	888.360470	12.209882
12.562032	878.752732	12.214899
12.248719	863.791188	12.219917
12.497184	866.923792	12.224935
12.314339	874.670927	12.229952
12.492649	862.901256	12.234970
12.745205	875.464704	12.239987
12.057387	869.469207	12.245005
12.591560	872.673572	12.250023
12.323255	881.530890	12.255040
12.134648	890.513599	12.260058
12.262158	902.291189	12.265075
12.465734	900.879888	12.270093
12.640484	893.227942	12.275111
12.636968	911.368351	12.280128
12.958048	898.567369	12.285146
12.750474	899.449589	12.290163
12.823412	888.024614	12.295181
12.921869	900.923827	12.300199
12.764495	895.434056	12.305216
12.777727	894.099576	12.310234
12.621255	898.565211	12.315251
13.189856	892.506733	12.320269
12.732364	879.433716	12.325287
12.664766	874.586082	12.330304
12.687831	859.469760	12.335322
12.979723	867.610201	12.340339
12.698054	871.200325	12.345357
12.630336	859.836601	12.350375
12.571163	862.636158	12.355392
13.052875	881.860303	12.360410
12.571127	875.240307	12.365427
12.688256	884.407878	12.370445
12.836538	881.936129	12.375463
12.981522	894.348996	12.380480
12.997924	891.559732	12.385498
12.906149	886.666000	12.390515
12.955114	884.452942	12.395533
13.197555	890.016512	12.400551
13.026242	876.622929	12.405568
12.776085	866.276273	12.410586
12.858688	867.794761	12.415603
12.789882	864.937216	12.420621
12.942402	882.995321	12.425639
13.147949	889.122463	12.430656
13.375933	872.576556	12.435674
12.873540	871.401586	12.440691
12.970375	861.563135	12.445709
13.266091	862.156609	12.450727
12.788885	860.136984	12.455744
12.904105	860.235973	12.460762
12.899174	869.198059	12.465779
13.026521	862.724808	12.470797
13.263181	881.194714	12.475815
12.913983	890.461591	12.480832
13.426801	877.068317	12.485850
12.687251	876.093629	12.490867
12.989799	889.616267	12.495885
13.316909	887.295543	12.500903
13.072918	898.861542	12.505920
13.121105	892.884735	12.510938
13.021909	897.638389	12.515955
12.986821	888.982927	12.520973
13.525071	885.695198	12.525991
13.003125	888.948430	12.531008
13.189876	885.441773	12.536026
13.326181	892.665986	12.541043
13.492931	883.581772	12.546061
13.575846	890.370204	12.551079
13.344834	895.027848	12.556096
13.472775	884.945113	12.561114
13.207164	876.163412	12.566131
13.102218	872.727892	12.571149
13.281418	872.208153	12.576167
13.316850	891.457546	12.581184
13.324140	885.570654	12.586202
13.191889	888.900209	12.591219
13.071673	882.765542	12.596237
12.975708	887.409033	12.601255
13.044497	888.966610	12.606272
13.265657	885.153732	12.611290
13.243447	886.646440	12.616307
13.093976	885.129734	12.621325
13.249450	890.738083	12.626343
13.349216	910.745526	12.631360
13.375736	922.128479	12.636378
13.569193	919.943497	12.641395
13.309420	927.672373	12.646413
13.379744	921.323853	12.651431
13.225895	926.599840	12.656448
13.493169	918.300226	12.661466
13.477962	918.113051	12.666483
13.388871	915.211810	12.671501
13.752812	924.703020	12.676519
13.724118	927.886753	12.681536
13.639528	918.804002	12.686554
13.854672	926.497988	12.691571
13.151877	927.400838	12.696589
13.719406	923.766200	12.701607
13.332121	927.747837	12.706624
13.534498	930.865437	12.711642
13.346021	921.948250	12.716659
13.300067	921.940336	12.721677
13.679148	918.539658	12.726695
13.460598	918.827640	12.731712
13.713581	942.705158	12.736730
14.261080	936.571622	12.741747
13.923605	932.538606	12.746765
14.328563	919.273532	12.751783
13.912475	925.431777	12.756800
13.867295	914.683466	12.761818
13.497851	912.046430	12.766835
13.695359	919.670999	12.771853
14.024914	913.646997	12.776871
14.253461	911.877794	12.781888
14.047894	913.224952	12.786906
13.921603	915.655463	12.791923
13.834732	909.071458	12.796941
14.296602	916.901013	12.801959
13.714676	917.579693	12.806976
14.126534	905.502054	12.811994
13.712263	914.489004	12.817011
13.756043	912.160088	12.822029
14.151689	907.740522	12.827047
13.487282	908.843781	12.832064
13.865364	901.215797	12.837082
13.692519	917.410837	12.842099
13.955458	918.550773	12.847117
14.159822	919.934402	12.852135
13.924574	915.540760	12.857152
13.841002	917.353496	12.862170
13.880081	918.797700	12.867187
13.761826	951.790448	12.872205
14.170739	940.028960	12.877223
14.292672	940.005898	12.882240
14.494293	954.475714	12.887258
14.468561	937.544676	12.892275
14.062828	923.547978	12.897293
14.166884	905.479588	12.902311
13.854551	912.790842	12.907328
14.162024	905.936885	12.912346
14.124923	930.151836	12.917363
13.903112	936.656061	12.922381
14.432196	956.192000	12.927399
14.444549	941.995312	12.932416
14.141780	940.713345	12.937434
14.471687	952.975839	12.942451
14.056185	956.810697	12.947469
14.109565	954.765570	12.952487
14.409939	954.364264	12.957504
14.714180	952.728683	12.962522
14.776601	954.209085	12.967539
14.124726	937.436726	12.972557
14.409979	921.673089	12.977575
14.576851	928.352996	12.982592
13.957760	930.961780	12.987610
14.478202	926.113687	12.992627
14.602308	955.650871	12.997645
14.095793	947.161159	13.002663
14.440327	950.974039	13.007680
14.692975	951.282069	13.012698
14.757868	949.017756	13.017715
14.340802	937.998268	13.022733
14.398289	946.634688	13.027751
14.701665	942.643081	13.032768
14.545394	948.555779	13.037786
14.714371	951.568391	13.042803
14.251216	948.027807	13.047821
14.937922	937.812253	13.052839
14.690606	934.318961	13.057856
14.326765	927.494648	13.062874
14.518341	932.626267	13.067891
14.435716	946.399680	13.072909
14.841266	940.372556	13.077927
14.746704	945.918820	13.082944
14.914655	952.240750	13.087962
15.013770	939.109848	13.092979
14.621553	935.091289	13.097997
14.897790	924.854911	13.103015
14.362663	916.817796	13.108032
14.747972	928.222451	13.113050
15.024019	931.511308	13.118067
14.385350	932.364198	13.123085
14.469941	940.440528	13.128103
14.647784	940.066458	13.133120
14.430245	939.938501	13.138138
14.990173	936.981372	13.143155
14.823021	950.450015	13.148173
15.164431	943.371575	13.153191
14.887795	946.506931	13.158208
14.864723	952.177579	13.163226
14.931784	951.412146	13.168243
14.649128	956.970800	13.173261
14.474045	949.286693	13.178279
14.753748	948.471556	13.183296
14.786553	941.081976	13.188314
14.987950	946.483876	13.193331
14.669472	948.111460	13.198349
14.847084	938.041836	13.203367
14.665081	940.682407	13.208384
14.809026	945.740125	13.213402
14.940755	961.494496	13.218419
15.168633	987.214978	13.223437
15.479918	965.181377	13.228455
15.244610	958.961288	13.233472
14.781302	959.478069	13.238490
15.025519	951.510141	13.243507
15.068686	969.725174	13.248525
15.452110	977.130695	13.253543
15.508672	945.387808	13.258560
14.910714	942.602835	13.263578
15.297006	950.926306	13.268595
15.234241	947.047262	13.273613
15.013638	944.861424	13.278631
14.849749	953.226514	13.283648
14.786982	962.904975	13.288666
15.037045	956.447028	13.293683
14.779564	978.083294	13.298701
15.190115	983.616657	13.303719
15.514910	974.284756	13.308736
15.105545	977.427489	13.313754
15.493500	985.623561	13.318771
14.965480	978.296727	13.323789
15.085714	971.758968	13.328807
15.481810	974.636825	13.333824
15.040150	987.322272	13.338842
15.705567	980.822049	13.343859
15.437836	977.640038	13.348877
15.797335	981.429689	13.353895
15.894726	976.332553	13.358912
15.552660	979.570051	13.363930
15.585234	980.186645	13.368947
15.543935	979.823006	13.373965
15.553505	976.063867	13.378983
15.385210	987.275654	13.384000
15.350015	986.117446	13.389018
15.585754	972.178644	13.394035
15.677841	981.018679	13.399053
15.718749	983.997452	13.404071
15.598337	964.442933	13.409088
15.411419	966.395369	13.414106
15.696615	981.977085	13.419123
15.478662	985.185217	13.424141
15.602550	977.895705	13.429159
15.499799	974.479086	13.434176
15.216601	982.454337	13.439194
15.550282	967.470698	13.444211
15.419417	979.064118	13.449229
15.415676	986.700131	13.454247
15.862489	988.007092	13.459264
15.999998	984.957781	13.464282
15.913039	993.655887	13.469299
15.715566	998.524614	13.474317
15.889510	979.979414	13.479335
15.802966	986.134396	13.484352
15.499533	990.001226	13.489370
16.051320	983.916559	13.494387
15.975067	993.297321	13.499405
15.806229	986.674278	13.504423
15.774126	969.985454	13.509440
15.978431	990.120876	13.514458
16.138812	981.122780	13.519475
15.903410	981.901256	13.524493
15.834549	976.254924	13.529511
16.243752	969.323312	13.534528
16.037451	974.648528	13.539546
15.916814	968.191709	13.544563
15.833251	958.666914	13.549581
16.197353	971.430669	13.554599
15.924083	967.710007	13.559616
16.007331	979.577634	13.564634
16.072324	980.191824	13.569651
16.259479	991.546314	13.574669
16.000629	985.910218	13.579687
16.128744	982.902020	13.584704
15.877987	993.710092	13.589722
16.047317	978.647617	13.594739
16.203516	983.799860	13.599757
16.090576	988.963714	13.604775
16.129886	985.594273	13.609792
15.760164	982.571512	13.614810
16.022453	995.226741	13.619827
15.893140	988.360594	13.624845
15.943896	991.408791	13.629863
15.942169	985.309413	13.634880
15.766524	1001.757223	13.639898
16.259476	989.452769	13.644915
17.018945	1011.732497	13.649933
16.867204	1002.963692	13.654951
17.127878	979.794836	13.659968
16.443767	989.364515	13.664986
16.702483	984.789339	13.670003
16.505645	976.573869	13.675021
16.512575	982.874792	13.680039
16.327224	976.392647	13.685056
16.493109	980.104864	13.690074
16.752131	978.256516	13.695091
16.765721	984.990809	13.700109
16.682947	982.562542	13.705127
16.656396	958.578147	13.710144
16.190732	960.105964	13.715162
16.589294	972.647037	13.720179
16.640969	973.506100	13.725197
16.672010	975.169808	13.730215
16.814300	969.023904	13.735232
16.445641	958.488833	13.740250
16.435283	953.824987	13.745267
16.808783	968.936962	13.750285
16.575883	971.665660	13.755303
16.802256	971.281601	13.760320
16.685917	973.302675	13.765338
16.623989	965.124060	13.770355
16.865025	963.256938	13.775373
16.470339	964.088601	13.780391
16.469386	968.458883	13.785408
16.907988	967.060893	13.790426
16.826859	978.565103	13.795443
16.925169	971.599154	13.800461
16.727494	975.176701	13.805479
16.816986	972.798989	13.810496
16.258142	973.575806	13.815514
16.774449	976.599419	13.820531
17.275969	977.790665	13.825549
17.070153	970.897017	13.830567
17.090539	980.251665	13.835584
16.698510	983.755741	13.840602
16.998079	973.417559	13.845619
16.918347	973.876366	13.850637
16.962913	979.605322	13.855655
17.206828	977.202975	13.860672
16.721427	984.872136	13.865690
16.827099	977.275453	13.870707
17.108635	976.558419	13.875725
16.871961	985.961652	13.880743
17.207761	974.790267	13.885760
16.845306	982.125188	13.890778
16.524940	977.039126	13.895795
17.078466	973.746099	13.900813
16.500180	973.520798	13.905831
17.026382	974.150682	13.910848
17.213736	991.584272	13.915866
16.952050	984.822172	13.920883
17.034353	980.578754	13.925901
16.846701	1005.330128	13.930919
17.244361	1009.831759	13.935936
17.318386	1019.726978	13.940954
17.033110	1014.099076	13.945971
17.497364	1019.287318	13.950989
17.295754	1023.563239	13.956007
17.418722	1004.433525	13.961024
17.037565	1006.932935	13.966042
16.942484	1016.452625	13.971059
17.445642	1010.537078	13.976077
16.993291	1015.812926	13.981095
17.251334	1017.042836	13.986112
17.566787	1014.692725	13.991130
17.307966	1009.807665	13.996147
17.069336	1010.850802	14.001165
17.140143	1026.419280	14.006183
17.615589	1005.558577	14.011200
17.288802	998.239613	14.016218
17.128864	1014.329786	14.021235
17.460273	1025.122171	14.026253
17.952923	1030.665800	14.031271
17.968023	1023.470411	14.036288
17.870600	1015.647278	14.041306
17.840484	1003.443325	14.046323
18.031321	997.739702	14.051341
17.712990	1013.169753	14.056359
17.798728	1011.536815	14.061376
17.480722	1000.640355	14.066394
17.104420	1002.162265	14.071411
17.401739	1000.019448	14.076429
17.397435	1005.319264	14.081447
17.678162	1005.510864	14.086464
17.777128	1026.894529	14.091482
17.613613	1030.383190	14.096499
18.002755	1022.117702	14.101517
17.552392	1029.480655	14.106535
18.141393	1028.898701	14.111552
18.452522	1020.185360	14.116570
18.134446	1014.975011	14.121587
18.328754	996.197823	14.126605
18.102836	989.620623	14.131623
17.694890	989.967360	14.136640
18.020031	1000.211255	14.141658
17.952183	996.696262	14.146675
18.272530	980.236336	14.151693
17.768543	994.690831	14.156711
17.776631	993.334854	14.161728
17.712185	998.859726	14.166746
17.608131	988.165474	14.171763
17.845426	986.068694	14.176781
17.732133	994.795755	14.181799
17.930853	1009.043012	14.186816
18.197466	1009.569464	14.191834
18.026713	1024.024617	14.196851
18.344920	1023.884686	14.201869
18.101810	1026.450444	14.206887
18.385222	1013.006788	14.211904
18.344374	1004.464102	14.216922
17.673928	1011.662467	14.221939
18.120819	1009.988939	14.226957
18.134341	1025.279334	14.231975
18.230141	1025.624406	14.236992
18.358528	1019.017869	14.242010
18.222397	1023.115774	14.247027
18.233524	1023.695271	14.252045
18.336711	1025.924815	14.257063
18.283994	1020.215968	14.262080
18.547721	1022.246571	14.267098
18.217674	1026.401714	14.272115
18.541361	1034.385343	14.277133
18.249752	1026.709039	14.282151
18.243858	1024.053038	14.287168
18.413099	1012.158003	14.292186
18.092673	1023.744599	14.297203
18.476408	1017.453972	14.302221
17.782206	1024.445578	14.307239
17.876572	1024.251808	14.312256
17.934815	1023.292685	14.317274
18.244142	1048.727811	14.322291
18.642328	1042.868077	14.327309
18.653199	1053.084527	14.332327
18.543474	1047.634555	14.337344
18.555081	1045.731433	14.342362
18.974819	1056.337128	14.347379
19.167071	1052.478207	14.352397
18.791725	1052.226944	14.357415
18.693663	1059.086788	14.362432
19.156747	1041.813877	14.367450
18.608757	1028.845239	14.372467
18.462550	1026.521919	14.377485
18.454715	1032.068643	14.382503
18.522801	1034.217488	14.387520
18.627988	1045.059278	14.392538
18.951935	1053.765977	14.397555
19.151167	1041.565227	14.402573
19.099300	1049.239829	14.407591
18.803184	1052.856099	14.412608
18.974564	1042.345978	14.417626
18.863435	1053.216435	14.422643
19.299790	1048.852788	14.427661
18.980701	1039.273180	14.432679
19.038754	1028.715666	14.437696
18.954960	1033.892136	14.442714
18.678951	1037.503603	14.447731
19.180068	1038.037555	14.452749
19.210540	1048.218190	14.457767
19.048940	1040.191907	14.462784
19.239821	1031.871791	14.467802
18.947552	1028.542867	14.472819
19.246626	1023.265758	14.477837
18.956931	1030.230965	14.482855
18.812979	1032.623475	14.487872
19.236855	1032.654337	14.492890
19.257623	1041.112560	14.497907
19.598329	1041.014967	14.502925
19.463934	1029.244196	14.507943
18.970294	1013.025818	14.512960
19.035084	998.162064	14.517978
18.874528	1020.767435	14.522995
19.189226	1030.411312	14.528013
19.354303	1028.177865	14.533031
19.257936	1040.282665	14.538048
19.547027	1035.939027	14.543066
19.180041	1049.332925	14.548083
19.261999	1037.003947	14.553101
19.304439	1045.476994	14.558119
19.084449	1037.729508	14.563136
19.335652	1029.393028	14.568154
19.320510	1047.446264	14.573171
19.312235	1037.394894	14.578189
19.355783	1043.073067	14.583207
19.342941	1034.198037	14.588224
19.437760	1032.682178	14.593242
19.390076	1046.139724	14.598259
19.623480	1041.966185	14.603277
19.644026	1046.295443	14.608295
19.271408	1044.460835	14.613312
19.563050	1049.329346	14.618330
19.479961	1061.250209	14.623347
19.522863	1070.459877	14.628365
19.697556	1062.428197	14.633383
19.844966	1064.157118	14.638400
19.761992	1063.305469	14.643418
19.679432	1064.059675	14.648435
19.539075	1069.296972	14.653453
19.652540	1067.278312	14.658471
19.691957	1069.488189	14.663488
19.938103	1060.681644	14.668506
19.590487	1066.096473	14.673523
19.626219	1063.842375	14.678541
19.740921	1059.312429	14.683559
19.672401	1072.122963	14.688576
20.081694	1061.560818	14.693594
19.697891	1067.422299	14.698611
19.808748	1072.864693	14.703629
19.696246	1061.253441	14.708647
19.776727	1062.006684	14.713664
20.315951	1061.421540	14.718682
20.059501	1065.855721	14.723699
19.997411	1069.083185	14.728717
20.142315	1072.377704	14.733735
19.843906	1064.634012	14.738752
19.803573	1058.660058	14.743770
20.087232	1079.452841	14.748787
20.213021	1085.714876	14.753805
20.584364	1090.551335	14.758823
19.993832	1076.488300	14.763840
20.281093	1072.049007	14.768858
20.112398	1077.002849	14.773875
20.261150	1084.034775	14.778893
20.545454	1072.913947	14.783911
20.228415	1071.387813	14.788928
20.452934	1064.254042	14.793946
20.095429	1066.149754	14.798963
20.282541	1073.110878	14.803981
20.800688	1084.370392	14.808999
20.035174	1083.135950	14.814016
20.245285	1084.114482	14.819034
20.326036	1085.097267	14.824051
20.584319	1089.637700	14.829069
20.726896	1086.251762	14.834087
20.485178	1064.696543	14.839104
20.848563	1055.436646	14.844122
20.225045	1062.006324	14.849139
20.375784	1044.658178	14.854157
20.830838	1060.450544	14.859175
20.379303	1058.096784	14.864192
20.456015	1052.917424	14.869210
20.383215	1060.094102	14.874227
20.472279	1071.445082	14.879245
20.600074	1087.265675	14.884263
20.400072	1085.113905	14.889280
20.978477	1073.806900	14.894298
20.332480	1088.441124	14.899315
20.377808	1092.060416	14.904333
20.975914	1080.089831	14.909351
20.575309	1098.486797	14.914368
20.831994	1082.486321	14.919386
20.972192	1084.618336	14.924403
21.035310	1090.947806	14.929421
20.941791	1086.774845	14.934439
21.164659	1088.361596	14.939456
21.113312	1086.636364	14.944474
20.897078	1077.660003	14.949491
20.611890	1079.704368	14.954509
20.813013	1079.153348	14.959527
20.528241	1086.628113	14.964544
20.622974	1077.747975	14.969562
20.846282	1088.555810	14.974579
20.534087	1085.751435	14.979597
20.989160	1076.794922	14.984615
20.776083	1094.772575	14.989632
21.234953	1101.594823	14.994650
21.253557	1107.270942	14.999667
21.145874	1106.857749	15.004685
21.479402	1103.765984	15.009703
21.360704	1100.903060	15.014720
21.460153	1085.835889	15.019738
21.148600	1084.925769	15.024755
21.326281	1082.735991	15.029773
21.520424	1077.609842	15.034791
21.011663	1079.189863	15.039808
21.080185	1075.575852	15.044826
21.288882	1077.105309	15.049843
21.149784	1073.417164	15.054861
21.107215	1077.527963	15.059879
20.944650	1104.131921	15.064896
21.267861	1105.189975	15.069914
21.581996	1106.123960	15.074931
21.333960	1110.724846	15.079949
21.685210	1107.097171	15.084967
21.204848	1131.032600	15.089984
21.328724	1114.518498	15.095002
21.443532	1106.958719	15.100019
21.623211	1112.903841	15.105037
21.742631	1108.563817	15.110055
21.631429	1114.278512	15.115072
21.666123	1115.351968	15.120090
21.625115	1107.209577	15.125107
21.473101	1121.654934	15.130125
22.004886	1107.789901	15.135143
21.696905	1112.629788	15.140160
21.492495	1113.326488	15.145178
21.567936	1110.235253	15.150195
21.410244	1119.088795	15.155213
21.615987	1104.521080	15.160231
21.870812	1109.680685	15.165248
21.758248	1101.193096	15.170266
22.080688	1111.075566	15.175283
21.924681	1105.415345	15.180301
21.776065	1098.285060	15.185319
21.421309	1109.726633	15.190336
21.591976	1101.578590	15.195354
21.787882	1108.454925	15.200371
21.532591	1136.645354	15.205389
21.987286	1134.646366	15.210407
22.337289	1136.099534	15.215424
22.168926	1136.720211	15.220442
22.208123	1119.169880	15.225459
21.795956	1116.806357	15.230477
22.237247	1115.819848	15.235495
21.959812	1128.122918	15.240512
22.115571	1131.718067	15.245530
22.644625	1121.515258	15.250547
22.159344	1112.233298	15.255565
22.333899	1102.978303	15.260583
21.741081	1095.558496	15.265600
22.070863	1098.623783	15.270618
22.330254	1123.019530	15.275635
22.276295	1125.730198	15.280653
22.509508	1120.575633	15.285671
22.341875	1131.732405	15.290688
22.594232	1129.151013	15.295706
22.654874	1121.529521	15.300723
22.257606	1110.783459	15.305741
22.189805	1103.526647	15.310759
22.604236	1107.834033	15.315776
22.579804	1111.417425	15.320794
22.597494	1098.066418	15.325811
22.312846	1100.563868	15.330829
22.363641	1101.642928	15.335847
22.421349	1122.389757	15.340864
22.552288	1121.010318	15.345882
22.404837	1122.639572	15.350899
22.111265	1129.089804	15.355917
22.299993	1130.417483	15.360935
22.166095	1129.852151	15.365952
22.395327	1122.915277	15.370970
22.493915	1123.665825	15.375987
22.317547	1115.044702	15.381005
22.605197	1130.276124	15.386023
22.810586	1157.233964	15.391040
22.921194	1151.574147	15.396058
23.077103	1147.765985	15.401075
23.039904	1155.062885	15.406093
23.144504	1132.351802	15.411111
23.390378	1132.735746	15.416128
23.122424	1139.284093	15.421146
23.085461	1125.809242	15.426163
23.210983	1121.793741	15.431181
23.254935	1116.336062	15.436199
23.177360	1120.697400	15.441216
23.132441	1118.800461	15.446234
22.977282	1116.478114	15.451251
23.063852	1115.822422	15.456269
23.092779	1114.310064	15.461287
23.163494	1117.741340	15.466304
22.787159	1110.364084	15.471322
22.881725	1111.786049	15.476339
22.635490	1106.956741	15.481357
22.832094	1108.151249	15.486375
23.140499	1113.945397	15.491392
22.633552	1119.626888	15.496410
23.183305	1123.038638	15.501427
23.000367	1140.956058	15.506445
23.402980	1141.164323	15.511463
23.149595	1138.874935	15.516480
23.283612	1152.448389	15.521498
23.640691	1144.300615	15.526515
23.304967	1139.978326	15.531533
23.554476	1135.174745	15.536551
23.325169	1135.952909	15.541568
23.144133	1141.900181	15.546586
23.484681	1142.532019	15.551603
23.265300	1151.714422	15.556621
22.994378	1136.603700	15.561639
23.381062	1139.098859	15.566656
23.341426	1146.898830	15.571674
23.078421	1134.305278	15.576691
23.122991	1151.991644	15.581709
23.395411	1174.991459	15.586727
23.715867	1159.816643	15.591744
23.500307	1176.766036	15.596762
23.724307	1168.988019	15.601779
23.744166	1164.629398	15.606797
23.713627	1169.332131	15.611815
23.933911	1167.343731	15.616832
23.874700	1166.049836	15.621850
23.908532	1170.024925	15.626867
24.091893	1173.265776	15.631885
24.225370	1164.056503	15.636903
24.100008	1159.486685	15.641920
23.640304	1170.771463	15.646938
24.046966	1154.640632	15.651955
24.224291	1167.665892	15.656973
23.963386	1165.444660	15.661991
24.011198	1162.591012	15.667008
23.755755	1158.154681	15.672026
23.880780	1172.595439	15.677043
23.582163	1163.083618	15.682061
23.849427	1161.042383	15.687079
24.105352	1164.221250	15.692096
24.044615	1164.600951	15.697114
24.135632	1152.900889	15.702131
24.181682	1159.575277	15.707149
24.275968	1149.621236	15.712167
24.248914	1155.581841	15.717184
24.021422	1171.948849	15.722202
24.213157	1162.981089	15.727219
24.417985	1166.231775	15.732237
24.308890	1166.040824	15.737255
24.362931	1159.969359	15.742272
24.199613	1162.511915	15.747290
24.232138	1160.972191	15.752307
24.543912	1156.721605	15.757325
24.331364	1152.997358	15.762343
24.512533	1161.316069	15.767360
24.319679	1169.057920	15.772378
25.228643	1175.242332	15.777395
24.747637	1161.545602	15.782413
24.450189	1148.665063	15.787431
24.627441	1146.172445	15.792448
24.005153	1164.733465	15.797466
24.295888	1162.854269	15.802483
24.716886	1176.357685	15.807501
24.822160	1186.277863	15.812519
24.946620	1182.436509	15.817536
24.955709	1187.698944	15.822554
24.820462	1172.748807	15.827571
24.724869	1172.353099	15.832589
24.407285	1187.112248	15.837607
24.891797	1181.730930	15.842624
24.954922	1193.313710	15.847642
24.879184	1186.279000	15.852659
24.981956	1173.835172	15.857677
24.736410	1183.745814	15.862695
24.903008	1189.900180	15.867712
25.367783	1184.442805	15.872730
25.227032	1183.891200	15.877747
24.927159	1178.511573	15.882765
25.045533	1180.543879	15.887783
25.235121	1174.671626	15.892800
24.729298	1186.932773	15.897818
25.020379	1180.545796	15.902835
25.012684	1183.010285	15.907853
24.928394	1188.454660	15.912871
25.053161	1189.093423	15.917888
24.671449	1182.997912	15.922906
24.983522	1180.208644	15.927923
25.346571	1188.219210	15.932941
25.183118	1181.077758	15.937959
25.139534	1181.301895	15.942976
25.416822	1186.563899	15.947994
25.244232	1175.723388	15.953011
25.420958	1179.611294	15.958029
25.327178	1173.916359	15.963047
25.359842	1183.648764	15.968064
25.236404	1196.576333	15.973082
25.517051	1204.085058	15.978099
25.606212	1211.466007	15.983117
25.670317	1218.216165	15.988135
25.906731	1198.969839	15.993152
25.622613	1180.880443	15.998170
26.021571	1178.502142	16.003187
26.048973	1177.708611	16.008205
25.569075	1180.987232	16.013223
25.952504	1170.720872	16.018240
25.815442	1166.333074	16.023258
25.800020	1176.517244	16.028275
25.715284	1170.994015	16.033293
25.262879	1178.869299	16.038311
25.832606	1176.430302	16.043328
25.708059	1188.965397	16.048346
25.579672	1171.752097	16.053363
25.937105	1176.152569	16.058381
25.633898	1178.694627	16.063399
25.975263	1187.025653	16.068416
25.913294	1206.336313	16.073434
26.292648	1205.273827	16.078451
26.434255	1204.321288	16.083469
25.948959	1192.174593	16.088487
26.103825	1179.266517	16.093504
25.745011	1178.343732	16.098522
25.990369	1194.825900	16.103539
26.089389	1201.942070	16.108557
26.139652	1208.932858	16.113575
26.173573	1209.105217	16.118592
26.087791	1202.455168	16.123610
26.369530	1208.153381	16.128627
26.678907	1208.656930	16.133645
26.023094	1208.944057	16.138663
26.504887	1207.371613	16.143680
26.047482	1217.875070	16.148698
26.078195	1218.761623	16.153715
26.069149	1207.005232	16.158733
25.976842	1207.212818	16.163751
25.987104	1206.073554	16.168768
26.181361	1213.860690	16.173786
26.459672	1196.842316	16.178803
26.638205	1216.174258	16.183821
26.462584	1224.118964	16.188839
26.634512	1206.730229	16.193856
26.452517	1222.735304	16.198874
26.578708	1229.671828	16.203891
26.605971	1229.247156	16.208909
26.556723	1240.764894	16.213927
26.872374	1229.369919	16.218944
26.704702	1227.661138	16.223962
26.923981	1225.128890	16.228979
27.283235	1221.830915	16.233997
27.097011	1219.523921	16.239015
27.090908	1204.265450	16.244032
26.917689	1206.655541	16.249050
26.924974	1195.194049	16.254067
26.708707	1196.622513	16.259085
26.704153	1203.577877	16.264103
26.807863	1197.846163	16.269120
26.957069	1208.983895	16.274138
26.912324	1195.976530	16.279155
26.835043	1199.890671	16.284173
26.548535	1222.739459	16.289191
27.110799	1228.903641	16.294208
27.229804	1233.809400	16.299226
27.032772	1231.132203	16.304243
27.308913	1228.727543	16.309261
27.048340	1224.400880	16.314279
27.164740	1229.586354	16.319296
26.835213	1230.854827	16.324314
26.930963	1227.297099	16.329331
27.122827	1224.837087	16.334349
27.200233	1236.792676	16.339367
27.025478	1234.970713	16.344384
27.094978	1237.374430	16.349402
27.096923	1253.939990	16.354419
27.647899	1254.243602	16.359437
27.360079	1259.143382	16.364455
27.263433	1259.225525	16.369472
27.669158	1250.109377	16.374490
27.839060	1254.770550	16.379507
27.741938	1249.990559	16.384525
27.277685	1254.916345	16.389543
27.503980	1253.876198	16.394560
27.915847	1257.782933	16.399578
27.873958	1257.352958	16.404595
27.959195	1256.486688	16.409613
27.658521	1255.343497	16.414631
28.245807	1244.972545	16.419648
27.732539	1247.130891	16.424666
27.773027	1254.099302	16.429683
27.988030	1243.535189	16.434701
27.982184	1247.344639	16.439719
28.202544	1234.563664	16.444736
27.963715	1224.402854	16.449754
27.589136	1213.550034	16.454771
27.812004	1226.793568	16.459789
27.847249	1241.547014	16.464807
27.966758	1246.646364	16.469824
27.906126	1247.821592	16.474842
27.572494	1259.296196	16.479859
27.932503	1244.648336	16.484877
27.749728	1255.454410	16.489895
28.134391	1244.601081	16.494912
27.973394	1249.522216	16.499930
28.038825	1253.946363	16.504947
28.435943	1241.286739	16.509965
28.177293	1248.717114	16.514983
28.408468	1254.637839	16.520000
28.272806	1265.030294	16.525018
28.220363	1273.255803	16.530035
28.442279	1278.212866	16.535053
28.408462	1273.526327	16.540071
28.627918	1270.889728	16.545088
28.827110	1265.463617	16.550106
28.629248	1252.079406	16.555123
28.671326	1233.992333	16.560141
28.504071	1245.206399	16.565159
28.754735	1236.112145	16.570176
28.738088	1232.044728	16.575194
28.387062	1242.279481	16.580211
28.776195	1237.253615	16.585229
28.378368	1237.062943	16.590247
28.560969	1232.371947	16.595264
28.790758	1240.234511	16.600282
28.708511	1246.089526	16.605299
28.424848	1250.747710	16.610317
28.787799	1265.935333	16.615335
28.552512	1266.513540	16.620352
29.040984	1258.819705	16.625370
28.794135	1270.217585	16.630387
29.252741	1265.511278	16.635405
29.173685	1264.457427	16.640423
29.161799	1272.792357	16.645440
29.576954	1265.822726	16.650458
29.368210	1248.829081	16.655475
29.298574	1240.999174	16.660493
29.161888	1240.502989	16.665511
28.850530	1225.879885	16.670528
29.188824	1213.676586	16.675546
29.067922	1237.111315	16.680563
29.463082	1231.409366	16.685581
29.158089	1234.095209	16.690599
29.074337	1246.695448	16.695616
29.329566	1248.389647	16.700634
29.300630	1256.880904	16.705651
29.580587	1262.894539	16.710669
29.356290	1270.742605	16.715687
29.272296	1259.626609	16.720704
29.321008	1261.312817	16.725722
29.168124	1274.354749	16.730739
29.536661	1256.360134	16.735757
29.437408	1267.727520	16.740775
29.168040	1267.630759	16.745792
29.559367	1259.284186	16.750810
29.165023	1273.269418	16.755827
29.343238	1258.958033	16.760845
29.587540	1267.320692	16.765863
29.430557	1283.223483	16.770880
29.670319	1278.369114	16.775898
29.718076	1301.118299	16.780915
29.803625	1293.720916	16.785933
29.896404	1291.478024	16.790951
29.851449	1295.053829	16.795968
30.155821	1295.335802	16.800986
29.960679	1303.504409	16.806003
29.944476	1292.385453	16.811021
29.839577	1288.701051	16.816039
29.767297	1297.476024	16.821056
30.061636	1282.018834	16.826074
29.811708	1298.238921	16.831091
30.212869	1293.016395	16.836109
29.981869	1290.604995	16.841127
30.149542	1280.625949	16.846144
30.115039	1285.749582	16.851162
30.030556	1281.754573	16.856179
30.104719	1286.664611	16.861197
29.949014	1291.380389	16.866215
29.934594	1293.028616	16.871232
30.377135	1290.339600	16.876250
30.074619	1296.446945	16.881267
30.292711	1297.952042	16.886285
30.505716	1301.583432	16.891303
30.201941	1298.912053	16.896320
30.477704	1296.449778	16.901338
30.956151	1298.210819	16.906355
30.817916	1296.711502	16.911373
30.745946	1302.781932	16.916391
30.570640	1303.544292	16.921408
30.601026	1284.512980	16.926426
30.263011	1289.861546	16.931443
30.632296	1292.108859	16.936461
30.788124	1298.959821	16.941479
30.600799	1301.505186	16.946496
30.688236	1300.338990	16.951514
30.471688	1299.473974	16.956531
30.373781	1299.390406	16.961549
30.294823	1297.389048	16.966567
30.375447	1291.713273	16.971584
30.852211	1309.261677	16.976602
30.705788	1328.301648	16.981619
31.226382	1328.565015	16.986637
31.525878	1328.103422	16.991655
31.249881	1315.557727	16.996672
31.509952	1307.209004	17.001690
31.087236	1287.939817	17.006707
30.918459	1295.555332	17.011725
31.090989	1292.731633	17.016743
31.223336	1297.840490	17.021760
31.213325	1291.851397	17.026778
30.916737	1301.096443	17.031795
31.170862	1313.398026	17.036813
31.299820	1332.893205	17.041831
31.095369	1323.267313	17.046848
31.818204	1319.656321	17.051866
31.215952	1324.406146	17.056883
31.578099	1332.687367	17.061901
31.713354	1328.926267	17.066919
31.259297	1326.361595	17.071936
31.794211	1322.633452	17.076954
31.779271	1330.493008	17.081971
31.832479	1315.638733	17.086989
31.504518	1307.983350	17.092007
31.751552	1319.547053	17.097024
31.966010	1316.833528	17.102042
31.694498	1311.367094	17.107059
31.497413	1319.766310	17.112077
31.728740	1315.575622	17.117095
31.616554	1319.263117	17.122112
31.816052	1317.046082	17.127130
31.372220	1323.390734	17.132147
31.534780	1317.491598	17.137165
31.569178	1317.421792	17.142183
31.394541	1308.237172	17.147200
31.822536	1331.580748	17.152218
31.987446	1345.727328	17.157235
32.089426	1341.026200	17.162253
32.402265	1351.133410	17.167271
31.774147	1349.775662	17.172288
32.294965	1339.497903	17.177306
32.332592	1353.514957	17.182323
31.789504	1350.436924	17.187341
31.960934	1350.238780	17.192359
31.834440	1351.361917	17.197376
32.521883	1344.123470	17.202394
32.103305	1349.202146	17.207411
32.173362	1343.748535	17.212429
32.503584	1350.482920	17.217447
32.513393	1343.650700	17.222464
32.237121	1342.364712	17.227482
32.632643	1348.725369	17.232499
32.328899	1336.750690	17.237517
32.513262	1345.824959	17.242535
32.602562	1364.643373	17.247552
32.549584	1366.978387	17.252570
33.093586	1373.250157	17.257587
32.860299	1361.538577	17.262605
32.970977	1348.605974	17.267623
32.580770	1337.172667	17.272640
32.799010	1328.889694	17.277658
32.940965	1330.767359	17.282675
33.018939	1321.930099	17.287693
32.695240	1331.417205	17.292711
32.924086	1338.005370	17.297728
32.590834	1335.333738	17.302746
32.651322	1343.102107	17.307763
32.993190	1351.809657	17.312781
33.020350	1352.021909	17.317799
32.834498	1364.611955	17.322816
33.316771	1359.310658	17.327834
33.112286	1356.111522	17.332851
33.251035	1366.675792	17.337869
33.761741	1350.990484	17.342887
33.311771	1368.541731	17.347904
33.048237	1358.959039	17.352922
33.454189	1362.756167	17.357939
33.122853	1377.752381	17.362957
33.497336	1362.404486	17.367975
33.449079	1361.095577	17.372992
33.150238	1370.078675	17.378010
33.237170	1354.687375	17.383027
33.357736	1368.718095	17.388045
33.627280	1356.865165	17.393063
33.490343	1364.241432	17.398080
33.661390	1356.969042	17.403098
33.475010	1360.629247	17.408115
33.091262	1369.551781	17.413133
33.176815	1366.616083	17.418151
33.404283	1378.003563	17.423168
33.610710	1394.797648	17.428186
33.916205	1390.836379	17.433203
33.875400	1389.081028	17.438221
33.880953	1382.635460	17.443239
34.199416	1382.950535	17.448256
34.194505	1374.018494	17.453274
34.330557	1382.927961	17.458291
34.198269	1390.276114	17.463309
34.242294	1370.518142	17.468327
33.899968	1378.558772	17.473344
33.866414	1385.434377	17.478362
34.389538	1386.823337	17.483379
34.152020	1386.144627	17.488397
34.197443	1377.665024	17.493415
33.911560	1383.121131	17.498432
33.679282	1373.707648	17.503450
33.985139	1372.547078	17.508467
34.208742	1374.800173	17.513485
34.311736	1374.148251	17.518503
34.256723	1373.026650	17.523520
34.365396	1377.327169	17.528538
34.195218	1383.231998	17.533555
34.089979	1392.817665	17.538573
34.701032	1412.977063	17.543591
34.568522	1427.839107	17.548608
35.064463	1410.926441	17.553626
35.143337	1401.047411	17.558643
35.067757	1393.764783	17.563661
34.995583	1369.840032	17.568679
35.069993	1363.054600	17.573696
35.152612	1373.179793	17.578714
34.985822	1362.466715	17.583731
34.684030	1372.089180	17.588749
34.860360	1370.211545	17.593767
34.637902	1369.361475	17.598784
34.848012	1371.646125	17.603802
34.945665	1367.444054	17.608819
34.879355	1363.343477	17.613837
34.907277	1361.124085	17.618855
34.726572	1369.262393	17.623872
34.522081	1379.467511	17.628890
35.260904	1384.828879	17.633907
34.987012	1394.762645	17.638925
35.274912	1397.368449	17.643943
35.371093	1399.384769	17.648960
35.049350	1396.171542	17.653978
35.638461	1395.035412	17.658995
35.674376	1403.035594	17.664013
35.772486	1393.676737	17.669031
35.702301	1384.439973	17.674048
35.442266	1374.973407	17.679066
35.325493	1366.148426	17.684083
35.242729	1369.910980	17.689101
35.555678	1385.123715	17.694119
35.743956	1404.060052	17.699136
35.733454	1398.176692	17.704154
35.929922	1384.290259	17.709171
35.714939	1396.675336	17.714189
35.828675	1383.895521	17.719207
35.743123	1393.318313	17.724224
35.872046	1395.168027	17.729242
36.295046	1382.873836	17.734259
36.112729	1376.386886	17.739277
35.809527	1373.789206	17.744295
35.366593	1362.169938	17.749312
35.678707	1368.759118	17.754330
36.031807	1377.683691	17.759347
35.862164	1385.007704	17.764365
35.698898	1381.553757	17.769383
36.006053	1389.437270	17.774400
35.629609	1384.254054	17.779418
36.069807	1372.377438	17.784435
36.089333	1394.524237	17.789453
36.313117	1403.845531	17.794471
36.820147	1410.012420	17.799488
36.349597	1412.320594	17.804506
36.371208	1388.402951	17.809523
36.302719	1387.921471	17.814541
36.252842	1401.026791	17.819559
36.565940	1406.923803	17.824576
36.394837	1413.590099	17.829594
36.244930	1414.136882	17.834611
36.034190	1415.306420	17.839629
36.539234	1410.287915	17.844647
36.121833	1411.973225	17.849664
36.182859	1423.873210	17.854682
36.769912	1413.102442	17.859699
36.482564	1439.113815	17.864717
36.897658	1436.090974	17.869735
36.896131	1436.386499	17.874752
36.877390	1447.451976	17.879770
37.117785	1443.088914	17.884787
36.837308	1436.360718	17.889805
36.918725	1447.510022	17.894823
37.172514	1434.018934	17.899840
37.111303	1443.243473	17.904858
37.186440	1439.345845	17.909875
36.923380	1443.547797	17.914893
37.201288	1443.754238	17.919911
37.210177	1441.346079	17.924928
37.375415	1440.808063	17.929946
37.641178	1430.866245	17.934963
37.535712	1434.095639	17.939981
37.485129	1424.025814	17.944999
37.577408	1425.258254	17.950016
37.467158	1411.651976	17.955034
37.376394	1398.666215	17.960051
37.112949	1409.990377	17.965069
37.544736	1419.955750	17.970087
37.479431	1430.917116	17.975104
37.484768	1442.663548	17.980122
37.470838	1422.515932	17.985139
37.503726	1422.820925	17.990157
37.165309	1443.590545	17.995175
37.531568	1437.845273	18.000192
37.319183	1420.612114	18.005210
37.498237	1434.708218	18.010227
37.995439	1461.992726	18.015245
37.871337	1469.851497	18.020263
38.226815	1462.102189	18.025280
38.120007	1464.173516	18.030298
37.933135	1464.904138	18.035315
38.031689	1461.093370	18.040333
38.008211	1453.178967	18.045351
37.952737	1458.335843	18.050368
38.116316	1469.244651	18.055386
38.346840	1458.788439	18.060403
37.894359	1462.421786	18.065421
37.974941	1461.917637	18.070439
38.455046	1458.328029	18.075456
38.121510	1459.417680	18.080474
38.135445	1463.719118	18.085491
38.130239	1466.718005	18.090509
38.210967	1452.595753	18.095527
38.345641	1469.020535	18.100544
38.326515	1482.104900	18.105562
38.421774	1486.477734	18.110579
38.525142	1490.048559	18.115597
38.429695	1489.420569	18.120615
38.847431	1489.098858	18.125632
38.437808	1489.678327	18.130650
38.457200	1491.133810	18.135667
38.580255	1484.811674	18.140685
38.878361	1486.317935	18.145703
38.727384	1482.422038	18.150720
38.669514	1482.915233	18.155738
39.094941	1505.393482	18.160755
39.105753	1516.500182	18.165773
39.271007	1504.617135	18.170791
39.160567	1494.167448	18.175808
39.180182	1495.604788	18.180826
39.438778	1482.809416	18.185843
39.522005	1481.809036	18.190861
39.318733	1485.213831	18.195879
39.355853	1483.255856	18.200896
39.392452	1481.289307	18.205914
39.763786	1472.486345	18.210931
39.291847	1477.046201	18.215949
39.238913	1486.170396	18.220967
39.367674	1476.786347	18.225984
39.107970	1482.118692	18.231002
39.452388	1479.168340	18.236019
39.411863	1498.040060	18.241037
39.162599	1507.969828	18.246055
39.463324	1501.362653	18.251072
39.502319	1515.223352	18.256090
39.595500	1498.502129	18.261107
39.860298	1502.469644	18.266125
39.818521	1505.692070	18.271143
39.780922	1501.947290	18.276160
39.837041	1509.960722	18.281178
40.133758	1508.309991	18.286195
39.926792	1490.039000	18.291213
39.715720	1500.795206	18.296231
39.897303	1503.408560	18.301248
39.419718	1516.361855	18.306266
39.832012	1509.776785	18.311283
40.084028	1529.442008	18.316301
40.475698	1542.624265	18.321319
40.493923	1524.635463	18.326336
40.589309	1531.848633	18.331354
40.851328	1524.077932	18.336371
40.575796	1512.079755	18.341389
40.375921	1507.625280	18.346407
40.648404	1493.091437	18.351424
40.161069	1492.106023	18.356442
40.350448	1494.230756	18.361459
40.211598	1505.453505	18.366477
40.195707	1510.287171	18.371495
40.686373	1526.592171	18.376512
40.696834	1538.709430	18.381530
41.022696	1529.746257	18.386547
40.984288	1540.624920	18.391565
40.585204	1545.802392	18.396583
40.657354	1529.686100	18.401600
40.767589	1532.901914	18.406618
40.539249	1531.381838	18.411635
40.727673	1532.722791	18.416653
40.386218	1530.173329	18.421671
41.014062	1524.926846	18.426688
41.060754	1529.361058	18.431706
40.998891	1552.170850	18.436723
41.302094	1548.671863	18.441741
41.397148	1558.142853	18.446759
41.759161	1554.060211	18.451776
41.319983	1548.847351	18.456794
41.256506	1527.530392	18.461811
41.582166	1527.965721	18.466829
41.291846	1530.237240	18.471847
41.465187	1513.280935	18.476864
41.368235	1529.763937	18.481882
41.545910	1541.491216	18.486899
41.704502	1545.605409	18.491917
41.396316	1542.729626	18.496935
41.730815	1536.791169	18.501952
41.758266	1540.391477	18.506970
42.116098	1547.269791	18.511987
41.914986	1546.441573	18.517005
41.518754	1544.743365	18.522023
41.759406	1542.234695	18.527040
41.525252	1549.362783	18.532058
41.631221	1540.700865	18.537075
41.408475	1545.857069	18.542093
41.133424	1549.875230	18.547111
41.965984	1554.411835	18.552128
41.879323	1556.896715	18.557146
41.760899	1566.197111	18.562163
42.009869	1565.280738	18.567181
41.720394	1575.841517	18.572199
42.238999	1574.385183	18.577216
42.217563	1569.596718	18.582234
42.172167	1567.296512	18.587251
42.377633	1567.700924	18.592269
42.195684	1577.232266	18.597287
42.501986	1588.021326	18.602304
42.722371	1590.543650	18.607322
42.852210	1599.626489	18.612339
42.816549	1562.798761	18.617357
42.341691	1562.835940	18.622375
42.701711	1557.151095	18.627392
42.758033	1581.125879	18.632410
42.813483	1581.541107	18.637427
43.085440	1592.054587	18.642445
42.832878	1578.901146	18.647463
42.728004	1555.389327	18.652480
42.865808	1563.888431	18.657498
43.046267	1585.755010	18.662515
43.387910	1587.180278	18.667533
42.889838	1588.893109	18.672551
43.215082	1587.252024	18.677568
43.270163	1596.202354	18.682586
43.348994	1595.962431	18.687603
43.115395	1578.800110	18.692621
43.231876	1591.855074	18.697639
43.357314	1593.729990	18.702656
43.528498	1596.792458	18.707674
43.625733	1591.316948	18.712691
43.691846	1583.391412	18.717709
43.086501	1572.986846	18.722727
42.808627	1572.187254	18.727744
43.093968	1586.506058	18.732762
43.647891	1585.932936	18.737779
43.870154	1584.335441	18.742797
43.603728	1592.506533	18.747815
43.485578	1577.944065	18.752832
43.887558	1581.258311	18.757850
43.604484	1585.785020	18.762867
43.646394	1586.458946	18.767885
43.782755	1603.683679	18.772903
43.745761	1616.087346	18.777920
43.972074	1627.813543	18.782938
44.181098	1620.437129	18.787955
44.211493	1604.903564	18.792973
44.253303	1611.312154	18.797991
44.435562	1608.281897	18.803008
44.572535	1614.214786	18.808026
44.212313	1612.016199	18.813043
44.781930	1600.590201	18.818061
44.420315	1594.600439	18.823079
44.224323	1583.298216	18.828096
44.481953	1590.479879	18.833114
44.251905	1609.085654	18.838131
44.561015	1610.203155	18.843149
44.303971	1606.869167	18.848167
44.460573	1608.580690	18.853184
44.218864	1611.838145	18.858202
44.076251	1617.272824	18.863219
44.524617	1604.538302	18.868237
44.439759	1617.049472	18.873255
44.613627	1626.095725	18.878272
45.019101	1628.906520	18.883290
44.614821	1636.360162	18.888307
45.047740	1636.824023	18.893325
44.721178	1635.302454	18.898343
44.789932	1639.964911	18.903360
44.848877	1639.072259	18.908378
44.479444	1630.413861	18.913395
44.801606	1645.729058	18.918413
44.960141	1652.648030	18.923431
45.203457	1653.287496	18.928448
45.632228	1658.124292	18.933466
45.601985	1653.600213	18.938483
45.544404	1649.345185	18.943501
45.586248	1654.107946	18.948519
45.637214	1660.042075	18.953536
45.664340	1659.829984	18.958554
45.690834	1667.113649	18.963571
45.758570	1654.656720	18.968589
45.830637	1657.331303	18.973607
45.826306	1663.628855	18.978624
45.846099	1656.663171	18.983642
45.916753	1650.153786	18.988659
46.327569	1646.309282	18.993677
45.763159	1630.171125	18.998695
45.476266	1631.068460	19.003712
45.834457	1631.194521	19.008730
45.467871	1648.523082	19.013747
45.554656	1653.460282	19.018765
45.697234	1658.557335	19.023783
45.744761	1655.346605	19.028800
45.831106	1664.299681	19.033818
45.944692	1682.381695	19.038835
46.211410	1680.424528	19.043853
46.311537	1681.096908	19.048871
46.157864	1683.030358	19.053888
46.340278	1682.638689	19.058906
46.514526	1677.554896	19.063923
46.592597	1681.181317	19.068941
46.781873	1688.737463	19.073959
46.774153	1680.869544	19.078976
46.916198	1670.985216	19.083994
46.548161	1690.509836	19.089011
46.739709	1679.630051	19.094029
46.832242	1674.743203	19.099047
46.717929	1681.637600	19.104064
47.049417	1668.155906	19.109082
46.850460	1668.837557	19.114099
47.227067	1670.732583	19.119117
47.026960	1661.833222	19.124135
47.309989	1664.672327	19.129152
47.225604	1661.311960	19.134170
47.103745	1663.212005	19.139187
47.461187	1668.305440	19.144205
47.473227	1676.914945	19.149223
47.351873	1670.073156	19.154240
47.613706	1663.558351	19.159258
47.196555	1670.405950	19.164275
47.387830	1671.106372	19.169293
47.530214	1691.173727	19.174311
47.352785	1689.384036	19.179328
47.746381	1684.042764	19.184346
47.831011	1701.178726	19.189363
47.734596	1696.107769	19.194381
47.458304	1696.089303	19.199399
47.662082	1695.551405	19.204416
47.674401	1690.338875	19.209434
47.493146	1689.879957	19.214451
47.526776	1694.327200	19.219469
47.748592	1700.911566	19.224487
47.761830	1708.663523	19.229504
47.771070	1716.092170	19.234522
48.277319	1726.684726	19.239539
48.150144	1725.154409	19.244557
48.028848	1719.658674	19.249575
48.143512	1717.608141	19.254592
48.827535	1716.129577	19.259610
48.535487	1716.694740	19.264627
48.562578	1710.155526	19.269645
48.350392	1712.057513	19.274663
48.342516	1721.812704	19.279680
48.613480	1720.764555	19.284698
48.312826	1721.449433	19.289715
48.493207	1713.774794	19.294733
48.626411	1731.483397	19.299751
48.157293	1716.579634	19.304768
48.246289	1722.633864	19.309786
48.639437	1746.525494	19.314803
48.642836	1740.632816	19.319821
49.065809	1748.048220	19.324839
48.790761	1754.915085	19.329856
49.005026	1735.777247	19.334874
49.030152	1749.762087	19.339891
48.515342	1754.320251	19.344909
48.825940	1738.679822	19.349927
48.768920	1748.725595	19.354944
49.387068	1754.229463	19.359962
49.220264	1772.546083	19.364979
49.336821	1771.932646	19.369997
49.211646	1772.633995	19.375015
49.487544	1764.909102	19.380032
49.613988	1760.004814	19.385050
49.511705	1771.798018	19.390067
50.146120	1767.014090	19.395085
50.113401	1757.306993	19.400103
49.371677	1776.928902	19.405120
49.843208	1760.698936	19.410138
49.594578	1753.376828	19.415155
49.757915	1757.491869	19.420173
49.964155	1759.766983	19.425191
49.846381	1749.892080	19.430208
49.888875	1753.990085	19.435226
50.083915	1775.946245	19.440243
50.017115	1760.455747	19.445261
50.367962	1756.251488	19.450279
50.041642	1769.021947	19.455296
50.152404	1763.633500	19.460314
50.349685	1760.502712	19.465331
50.056155	1765.701391	19.470349
50.499422	1771.721504	19.475367
50.542567	1793.336301	19.480384
50.716375	1790.361532	19.485402
50.638015	1780.741480	19.490419
50.693202	1787.299883	19.495437
50.690100	1781.847775	19.500455
50.762828	1787.829139	19.505472
50.615378	1775.542891	19.510490
50.482784	1785.250040	19.515507
50.574472	1771.596492	19.520525
51.156417	1778.528416	19.525543
50.622912	1791.305377	19.530560
51.109221	1786.504388	19.535578
50.945145	1775.801988	19.540595
50.830226	1781.537228	19.545613
51.104797	1785.875596	19.550631
50.811275	1790.104129	19.555648
51.063047	1797.723614	19.560666
51.268875	1806.208659	19.565683
51.194805	1814.013674	19.570701
51.177018	1810.392890	19.575719
50.885755	1816.780238	19.580736
51.257053	1804.242123	19.585754
51.650239	1813.094390	19.590771
51.519943	1821.232085	19.595789
51.832228	1818.037996	19.600807
51.762957	1825.430266	19.605824
51.925405	1832.969463	19.610842
51.881121	1814.784180	19.615859
51.878661	1809.794498	19.620877
51.867168	1807.802591	19.625895
51.774789	1816.232012	19.630912
51.997445	1822.669460	19.635930
52.019503	1839.069354	19.640947
52.010620	1847.797949	19.645965
52.479104	1827.104196	19.650983
52.354470	1838.306533	19.656000
52.537086	1826.614441	19.661018
52.674117	1835.499209	19.666035
52.531678	1819.605256	19.671053
52.469011	1799.446108	19.676071
52.240567	1804.599797	19.681088
52.551461	1811.490317	19.686106
52.512184	1824.638335	19.691123
52.344317	1837.382469	19.696141
52.764543	1828.396444	19.701159
52.656832	1832.780481	19.706176
52.652466	1842.640471	19.711194
52.730279	1831.827793	19.716211
52.520237	1830.792005	19.721229
52.552099	1826.596350	19.726247
52.790328	1826.985318	19.731264
52.637878	1831.522792	19.736282
52.837041	1848.195362	19.741299
52.949661	1857.858295	19.746317
53.065214	1858.611195	19.751335
52.945856	1859.267300	19.756352
53.243270	1862.816971	19.761370
53.275446	1849.372180	19.766387
53.122635	1859.401773	19.771405
53.132944	1874.780739	19.776423
53.338113	1876.453167	19.781440
53.750294	1880.458034	19.786458
53.772491	1881.175580	19.791475
54.001229	1882.548677	19.796493
53.949745	1871.443989	19.801511
53.821829	1882.194002	19.806528
54.053656	1873.623290	19.811546
54.166637	1867.747096	19.816563
53.923365	1875.584630	19.821581
54.096138	1879.446009	19.826599
53.696930	1875.672714	19.831616
54.012695	1878.696585	19.836634
53.941040	1888.902329	19.841651
53.836428	1877.104729	19.846669
54.107930	1863.928607	19.851687
54.202967	1882.210158	19.856704
54.575410	1882.942456	19.861722
54.635712	1885.103336	19.866739
54.100658	1887.449596	19.871757
54.705060	1884.939417	19.876775
54.729451	1899.720483	19.881792
54.495898	1905.113801	19.886810
55.112816	1901.825658	19.891827
54.627228	1903.233541	19.896845
54.899369	1893.080752	19.901863
54.682849	1907.916989	19.906880
54.718052	1905.199721	19.911898
55.115697	1892.791220	19.916915
54.768706	1911.665473	19.921933
54.952909	1890.394277	19.926951
55.229711	1892.959487	19.931968
55.126608	1913.965821	19.936986
54.862068	1905.215926	19.942003
54.807010	1903.353239	19.947021
55.478119	1914.305055	19.952039
55.096456	1929.404007	19.957056
55.198624	1923.482931	19.962074
55.519492	1924.042082	19.967091
55.392834	1924.591141	19.972109
55.416407	1926.095575	19.977127
55.726009	1922.670242	19.982144
55.675519	1924.892935	19.987162
55.980103	1922.371278	19.992179
55.496698	1928.284380	19.997197
55.754258	1911.193459	20.002215
55.728247	1925.456365	20.007232
55.778998	1940.174853	20.012250
55.842796	1942.782947	20.017267
56.302555	1945.692102	20.022285
56.102719	1949.445012	20.027303
56.164877	1936.672278	20.032320
56.183232	1942.255254	20.037338
56.255982	1939.433755	20.042355
56.150863	1944.832042	20.047373
56.589446	1954.305360	20.052391
56.874758	1941.108586	20.057408
56.567941	1938.666899	20.062426
56.890132	1944.562421	20.067443
56.695238	1940.665987	20.072461
56.926621	1936.761704	20.077479
56.765647	1943.044119	20.082496
57.278898	1938.921820	20.087514
56.897181	1941.815320	20.092531
56.849138	1936.660905	20.097549
56.981665	1944.081887	20.102567
57.064730	1939.190024	20.107584
57.032494	1942.308418	20.112602
57.337615	1934.829370	20.117619
56.857547	1943.337491	20.122637
57.122084	1953.003920	20.127655
57.163084	1968.301933	20.132672
57.291909	1972.398918	20.137690
57.536324	1972.199139	20.142707
57.532372	1966.915395	20.147725
57.651668	1964.395613	20.152743
57.768150	1972.360930	20.157760
57.486323	1968.740439	20.162778
57.771892	1959.782496	20.167795
57.809181	1976.236903	20.172813
58.012817	1964.925638	20.177831
57.812838	1967.615312	20.182848
57.915222	1962.485631	20.187866
58.332902	1956.900155	20.192883
57.606572	1963.192941	20.197901
58.007401	1957.296703	20.202919
57.898965	1975.853102	20.207936
58.131853	1987.535776	20.212954
58.466799	1979.534514	20.217971
58.149951	1986.066103	20.222989
58.346481	1978.664027	20.228007
58.354652	1980.376304	20.233024
58.554238	1988.601290	20.238042
58.834043	1986.625390	20.243059
58.223810	1996.782032	20.248077
58.555818	1984.618332	20.253095
58.804987	2013.746773	20.258112
59.045713	2014.034950	20.263130
59.010458	2010.558920	20.268147
59.131314	2009.824502	20.273165
59.418162	2011.533639	20.278183
59.366918	1987.620609	20.283200
59.207687	1973.552295	20.288218
59.259334	1967.773984	20.293235
59.075857	1967.151662	20.298253
59.311850	1977.642219	20.303271
59.119862	2001.242203	20.308288
58.983481	2005.670588	20.313306
59.384926	1998.686165	20.318323
59.491132	2006.909075	20.323341
59.452681	1998.226282	20.328359
59.718541	1988.509065	20.333376
59.559301	2004.282476	20.338394
59.789450	1995.553724	20.343411
59.590899	1998.788579	20.348429
59.525496	1999.359207	20.353447
59.642698	2016.922571	20.358464
59.733033	2016.012114	20.363482
59.958971	2027.223185	20.368499
59.905496	2030.776555	20.373517
60.099717	2032.299842	20.378535
60.358075	2022.304938	20.383552
59.912737	2034.327453	20.388570
59.990347	2016.329444	20.393587
60.373210	2050.423696	20.398605
60.483576	2052.981795	20.403623
60.535660	2055.475911	20.408640
60.302742	2069.305672	20.413658
60.489260	2061.125177	20.418675
60.917317	2061.839043	20.423693
60.746270	2054.984628	20.428711
60.860238	2053.201459	20.433728
60.338464	2056.612560	20.438746
60.720270	2045.412132	20.443763
60.855317	2069.437260	20.448781
61.143207	2074.038836	20.453799
61.575605	2073.283639	20.458816
61.020905	2089.091977	20.463834
61.078514	2078.747572	20.468851
61.206142	2079.080422	20.473869
61.288960	2071.376458	20.478887
61.620325	2077.105572	20.483904
61.791180	2068.411771	20.488922
61.706908	2069.654739	20.493939
61.183654	2078.015165	20.498957
61.525057	2077.628313	20.503975
61.669773	2075.199579	20.508992
61.712753	2086.541702	20.514010
61.758602	2089.869050	20.519027
61.910324	2101.870703	20.524045
62.116915	2110.814010	20.529063
62.372380	2104.092024	20.534080
62.206697	2100.113368	20.539098
62.562484	2098.351646	20.544115
62.635572	2099.809139	20.549133
62.687388	2100.795592	20.554151
62.799219	2089.811184	20.559168
62.264820	2077.406766	20.564186
62.284312	2073.928957	20.569203
62.444591	2082.218358	20.574221
62.546187	2085.625459	20.579239
62.548445	2097.412265	20.584256
62.489903	2100.666914	20.589274
62.910111	2084.566928	20.594291
62.814371	2094.092609	20.599309
62.601949	2096.166316	20.604327
62.490754	2086.677076	20.609344
62.818452	2115.192599	20.614362
62.763238	2118.827370	20.619379
62.720919	2115.526087	20.624397
63.123814	2118.800344	20.629415
63.677044	2124.322949	20.634432
63.181166	2121.663682	20.639450
63.403490	2115.386491	20.644467
63.279485	2112.384111	20.649485
63.226763	2125.641880	20.654503
63.735002	2129.463830	20.659520
63.710434	2154.620077	20.664538
63.986938	2140.589438	20.669555
63.886478	2142.589143	20.674573
63.992810	2148.711536	20.679591
64.325183	2143.508755	20.684608
64.209938	2145.896495	20.689626
64.002292	2119.674500	20.694643
64.048504	2124.844911	20.699661
64.067090	2142.202886	20.704679
64.804038	2129.544643	20.709696
64.423087	2140.504151	20.714714
64.500757	2144.430717	20.719731
64.611904	2149.001292	20.724749
64.585411	2141.819438	20.729767
64.756790	2139.993903	20.734784
64.363001	2145.678716	20.739802
64.434516	2133.726629	20.744819
64.426795	2135.430920	20.749837
64.705144	2143.331196	20.754855
64.937089	2133.806284	20.759872
64.616798	2137.720469	20.764890
64.705964	2142.254128	20.769907
64.961303	2154.551266	20.774925
64.766465	2149.599365	20.779943
64.924542	2158.197210	20.784960
65.127334	2163.492334	20.789978
65.154130	2161.072247	20.794995
64.710945	2173.642294	20.800013
64.905951	2178.131507	20.805031
65.646535	2180.389048	20.810048
65.528846	2194.773248	20.815066
65.348240	2199.523336	20.820083
65.627170	2189.955590	20.825101
65.589404	2182.785225	20.830119
66.061989	2186.880378	20.835136
66.074204	2193.473021	20.840154
66.086046	2191.697265	20.845171
66.353247	2192.883738	20.850189
65.894125	2186.684287	20.855207
66.324315	2204.287080	20.860224
66.072136	2222.405370	20.865242
66.423662	2208.608508	20.870259
66.936924	2201.643702	20.875277
66.713265	2216.267459	20.880295
67.195936	2210.827634	20.885312
66.888750	2192.644802	20.890330
66.614073	2177.052028	20.895347
66.708640	2179.467301	20.900365
66.872332	2175.413333	20.905383
67.091814	2181.105862	20.910400
66.778918	2198.375385	20.915418
66.944800	2199.457747	20.920435
67.002684	2195.400001	20.925453
66.787642	2207.814671	20.930471
66.899387	2206.217071	20.935488
67.020451	2204.218560	20.940506
66.861081	2201.674324	20.945523
66.992567	2212.121096	20.950541
67.100368	2232.769423	20.955559
66.931045	2233.660746	20.960576
67.330484	2229.744366	20.965594
67.731538	2242.844581	20.970611
67.722088	2233.927751	20.975629
67.334668	2231.227512	20.980647
68.047695	2244.467299	20.985664
67.991951	2261.503865	20.990682
67.974387	2261.052127	20.995699
68.246188	2254.954679	21.000717
68.084590	2263.761693	21.005735
68.302558	2243.834696	21.010752
67.789033	2250.823462	21.015770
68.104518	2248.408801	21.020787
68.177698	2242.232773	21.025805
68.409837	2246.618439	21.030823
68.379368	2249.288220	21.035840
68.798131	2248.480943	21.040858
68.404679	2243.909830	21.045875
68.885992	2236.866044	21.050893
68.765821	2251.977804	21.055911
68.892090	2240.818281	21.060928
68.914150	2268.546486	21.065946
69.002783	2273.733556	21.070963
69.277274	2272.974329	21.075981
68.892011	2285.825025	21.080999
69.060812	2278.818493	21.086016
69.144647	2277.078465	21.091034
68.879554	2283.648079	21.096051
69.178307	2281.383604	21.101069
69.414640	2284.680107	21.106087
69.612402	2280.216780	21.111104
69.479713	2279.836029	21.116122
69.621373	2312.357878	21.121139
69.823018	2302.808936	21.126157
69.633856	2313.813835	21.131175
69.702927	2307.802224	21.136192
69.489924	2305.160149	21.141210
69.820174	2303.031793	21.146227
70.263206	2308.689790	21.151245
69.917482	2316.027988	21.156263
70.205702	2321.588158	21.161280
70.382236	2331.741570	21.166298
70.312461	2337.813225	21.171315
70.653332	2333.632506	21.176333
70.382858	2338.622663	21.181351
70.602807	2335.797829	21.186368
70.697202	2330.660686	21.191386
70.451916	2326.997264	21.196403
71.066739	2334.469827	21.201421
70.853514	2330.885547	21.206439
70.996243	2318.397974	21.211456
70.964085	2315.013481	21.216474
71.233829	2312.517990	21.221491
71.588842	2319.297325	21.226509
71.204935	2330.244464	21.231527
71.244352	2329.123526	21.236544
70.995470	2336.012107	21.241562
71.482951	2346.434590	21.246579
71.659980	2345.631037	21.251597
71.606211	2347.549635	21.256615
71.830868	2358.332851	21.261632
71.939294	2345.497610	21.266650
71.663894	2351.565851	21.271667
72.071895	2347.455131	21.276685
71.536551	2351.911750	21.281703
71.677655	2346.036239	21.286720
71.886955	2353.925989	21.291738
71.694769	2355.152563	21.296755
72.055624	2367.598366	21.301773
72.336564	2382.121379	21.306791
72.275530	2372.077658	21.311808
72.462973	2371.767025	21.316826
72.286585	2378.249389	21.321843
72.352479	2366.524803	21.326861
72.069224	2370.135708	21.331879
72.231926	2374.289796	21.336896
72.828488	2386.787602	21.341914
72.541975	2413.200245	21.346931
73.007814	2401.543194	21.351949
72.781527	2400.355929	21.356967
73.009247	2393.420115	21.361984
73.106681	2396.602205	21.367002
73.074551	2402.745808	21.372019
73.479881	2390.881655	21.377037
73.258163	2404.147709	21.382055
73.308047	2398.972823	21.387072
73.402846	2404.872047	21.392090
73.380589	2415.039467	21.397107
73.482025	2425.398641	21.402125
73.943004	2430.838973	21.407143
73.760273	2424.755549	21.412160
73.792061	2415.094854	21.417178
73.799088	2430.505820	21.422195
73.606606	2415.746395	21.427213
73.852154	2433.486450	21.432231
74.222814	2441.931224	21.437248
74.512300	2441.916694	21.442266
74.328937	2446.840330	21.447283
74.441598	2443.065175	21.452301
74.355135	2442.512031	21.457319
74.419582	2453.879616	21.462336
74.649300	2446.152567	21.467354
74.645889	2452.811677	21.472371
74.679268	2440.897936	21.477389
74.805243	2452.684647	21.482407
74.801739	2446.881809	21.487424
74.714104	2436.779061	21.492442
74.807530	2466.773395	21.497459
75.037748	2475.998421	21.502477
75.096884	2466.855573	21.507495
75.183135	2459.704346	21.512512
75.245844	2468.121092	21.517530
74.962851	2457.926607	21.522547
75.060006	2466.159131	21.527565
75.371776	2499.545515	21.532583
75.455374	2500.880454	21.537600
75.861255	2493.295912	21.542618
75.760356	2492.759717	21.547635
76.080830	2478.182573	21.552653
75.988768	2489.302840	21.557671
76.180997	2494.191589	21.562688
76.326509	2483.715862	21.567706
76.009914	2485.506465	21.572723
76.303465	2493.534911	21.577741
76.469710	2503.972791	21.582759
76.414388	2511.752621	21.587776
76.692275	2513.684146	21.592794
76.827999	2524.740422	21.597811
77.485052	2507.031100	21.602829
76.832956	2502.503436	21.607847
76.683666	2489.458123	21.612864
77.122644	2474.805696	21.617882
76.688250	2484.059061	21.622899
77.173465	2498.258884	21.627917
76.934890	2511.215045	21.632935
77.029234	2518.284767	21.637952
77.115448	2521.718718	21.642970
77.085963	2533.106213	21.647987
77.370856	2518.840595	21.653005
77.241701	2526.496423	21.658023
77.110863	2519.952847	21.663040
77.416768	2530.165518	21.668058
77.365117	2549.292311	21.673075
77.476518	2544.557965	21.678093
77.819791	2546.969203	21.683111
77.450245	2547.145459	21.688128
77.843837	2540.160714	21.693146
77.828429	2555.424736	21.698163
78.458569	2568.287389	21.703181
78.304376	2569.847834	21.708199
78.466620	2574.863996	21.713216
78.461017	2571.283930	21.718234
78.409485	2576.193499	21.723251
78.615829	2563.686360	21.728269
78.746844	2578.530569	21.733287
78.743014	2582.315215	21.738304
79.113218	2557.486445	21.743322
78.805708	2569.752917	21.748339
78.945913	2570.672830	21.753357
78.532505	2562.320556	21.758375
78.771227	2559.466401	21.763392
78.790896	2582.843334	21.768410
79.042914	2588.240896	21.773427
79.148784	2598.747278	21.778445
79.575549	2593.196096	21.783463
79.381116	2594.463609	21.788480
79.600139	2596.888694	21.793498
79.471928	2593.061778	21.798515
79.881707	2593.464936	21.803533
79.911136	2592.643835	21.808551
79.418329	2620.675451	21.813568
80.006621	2613.516975	21.818586
80.042763	2626.931737	21.823603
80.423500	2628.266402	21.828621
80.553617	2606.503194	21.833639
80.153000	2615.936869	21.838656
80.485730	2620.293423	21.843674
80.350494	2618.813556	21.848691
80.549061	2609.479485	21.853709
80.670398	2610.112972	21.858727
80.364290	2625.355026	21.863744
80.743601	2621.354086	21.868762
80.925032	2643.568242	21.873779
81.083725	2631.473618	21.878797
81.351570	2640.494901	21.883815
80.805425	2635.587904	21.888832
81.367306	2623.303835	21.893850
80.824258	2639.229892	21.898867
81.148622	2636.640685	21.903885
81.434924	2628.704998	21.908903
81.292285	2635.727523	21.913920
81.830885	2644.841460	21.918938
81.348340	2660.347924	21.923955
81.633420	2673.408817	21.928973
81.985917	2674.302316	21.933991
81.898106	2669.086515	21.939008
81.913613	2660.962307	21.944026
81.644569	2671.574192	21.949043
81.965967	2674.598276	21.954061
82.267768	2661.846559	21.959079
82.217851	2680.260679	21.964096
82.057674	2691.999392	21.969114
82.079492	2690.425067	21.974131
82.201893	2691.682158	21.979149
82.546514	2689.354341	21.984167
82.459411	2701.891169	21.989184
82.763911	2714.566236	21.994202
82.947066	2716.941169	21.999219
83.082797	2723.527997	22.004237
83.701780	2713.441169	22.009255
83.415073	2718.426059	22.014272
83.348746	2710.810394	22.019290
83.513480	2694.192579	22.024307
83.410604	2684.361068	22.029325
83.935206	2695.549453	22.034343
83.515376	2692.443293	22.039360
83.544979	2676.520616	22.044378
83.332826	2690.111887	22.049395
83.643950	2700.092327	22.054413
83.986287	2705.697432	22.059431
84.040742	2712.425827	22.064448
83.964116	2702.067953	22.069466
83.942278	2714.311742	22.074483
83.599889	2711.927575	22.079501
84.172752	2717.159967	22.084519
84.436236	2715.566373	22.089536
84.881148	2726.891170	22.094554
84.693377	2718.055885	22.099571
84.470672	2722.745180	22.104589
84.523914	2729.876512	22.109607
84.473273	2722.901908	22.114624
84.734868	2716.993553	22.119642
84.727349	2724.771299	22.124659
84.424179	2737.465899	22.129677
84.541964	2745.081423	22.134695
84.692184	2751.893216	22.139712
84.979530	2755.786078	22.144730
85.571049	2759.401921	22.149747
85.318603	2782.827272	22.154765
86.051539	2776.229431	22.159783
85.608964	2780.135046	22.164800
85.692919	2767.854647	22.169818
85.841869	2768.456020	22.174835
86.060976	2765.501138	22.179853
86.458160	2773.206719	22.184871
86.186888	2781.918771	22.189888
86.373912	2768.067891	22.194906
86.490237	2761.305429	22.199923
86.226851	2776.735442	22.204941
86.506813	2763.263279	22.209959
86.466285	2767.289452	22.214976
86.609802	2764.954504	22.219994
86.617182	2765.156068	22.225011
86.521421	2772.778942	22.230029
86.840883	2787.685122	22.235047
86.677720	2793.252340	22.240064
86.787758	2791.866957	22.245082
86.619974	2796.619242	22.250099
86.755517	2809.079604	22.255117
87.045095	2815.977447	22.260135
86.954308	2830.901462	22.265152
86.917140	2825.210731	22.270170
87.246052	2822.128645	22.275187
87.245005	2847.701794	22.280205
87.738016	2852.211053	22.285223
87.524155	2858.332310	22.290240
87.931423	2845.178785	22.295258
87.929512	2852.596831	22.300275
88.234166	2853.726778	22.305293
88.227260	2844.781617	22.310311
87.509124	2856.811462	22.315328
88.027979	2870.666326	22.320346
88.386483	2873.327055	22.325363
88.289594	2876.436243	22.330381
88.975029	2875.458107	22.335399
89.071014	2872.553863	22.340416
89.427764	2861.282190	22.345434
89.249093	2859.231951	22.350451
89.235405	2868.221547	22.355469
89.349001	2863.521582	22.360487
89.335234	2861.142141	22.365504
89.337734	2873.205271	22.370522
89.658928	2859.808097	22.375539
89.213890	2874.610780	22.380557
89.495876	2865.418275	22.385575
89.654440	2860.391606	22.390592
89.652837	2863.831876	22.395610
89.664535	2862.756422	22.400627
89.621404	2865.301244	22.405645
89.832058	2857.612179	22.410663
89.634247	2859.033805	22.415680
89.596784	2876.444976	22.420698
89.990689	2883.706297	22.425715
89.802491	2897.047347	22.430733
90.007336	2892.736210	22.435751
90.125818	2906.479716	22.440768
90.172532	2908.988046	22.445786
90.318120	2918.676905	22.450803
90.357307	2928.440042	22.455821
90.613254	2918.976625	22.460839
90.556971	2933.630090	22.465856
90.891934	2947.558322	22.470874
91.192848	2943.514352	22.475891
91.091270	2951.012297	22.480909
91.113928	2948.167792	22.485927
91.216833	2951.691202	22.490944
91.304886	2949.478377	22.495962
91.493138	2946.539583	22.500979
91.410998	2975.161623	22.505997
91.900083	2970.162188	22.511015
91.822666	2989.395353	22.516032
92.013358	2982.121711	22.521050
91.968215	2966.175263	22.526067
92.189407	2978.262178	22.531085
92.167189	2964.277597	22.536103
92.142929	2967.425192	22.541120
91.939185	2968.100601	22.546138
92.387585	2977.362707	22.551155
92.148850	2991.805443	22.556173
92.718168	3008.197641	22.561191
92.826204	2996.291016	22.566208
93.171585	2988.695760	22.571226
93.571940	2990.825210	22.576243
93.477478	2989.773194	22.581261
93.480551	2984.853278	22.586279
93.662371	2985.280339	22.591296
93.608737	2996.557604	22.596314
93.777049	2978.362984	22.601331
93.351129	2984.924431	22.606349
93.819052	2985.353032	22.611367
93.914477	2985.693980	22.616384
93.620423	2983.276194	22.621402
93.671923	2993.370393	22.626419
93.852966	2990.348533	22.631437
93.788485	2980.567179	22.636455
93.766380	2995.129232	22.641472
93.506712	3014.163027	22.646490
93.745822	3006.763268	22.651507
93.607912	3024.634489	22.656525
93.841328	3045.008433	22.661543
94.455010	3043.331546	22.666560
94.319560	3041.999304	22.671578
94.500653	3041.934777	22.676595
94.642719	3069.889263	22.681613
94.834667	3076.194326	22.686631
94.906342	3074.547552	22.691648
95.050816	3081.782470	22.696666
95.247018	3066.325151	22.701683
95.329040	3074.370351	22.706701
95.142567	3077.111721	22.711719
95.550588	3076.088868	22.716736
95.536874	3095.487222	22.721754
95.706776	3104.402526	22.726771
95.722883	3093.774746	22.731789
95.579550	3093.535096	22.736807
95.835208	3105.580590	22.741824
96.014956	3097.025683	22.746842
96.251922	3095.752759	22.751859
95.994611	3087.756278	22.756877
96.133327	3102.599720	22.761895
96.588708	3113.587456	22.766912
96.348291	3116.051143	22.771930
96.542032	3119.641075	22.776947
96.553510	3114.749648	22.781965
96.436777	3119.199512	22.786983
96.761409	3132.523343	22.792000
96.433706	3145.342403	22.797018
97.091635	3130.408700	22.802035
97.145121	3142.282520	22.807053
97.416185	3140.882703	22.812071
97.498433	3139.971155	22.817088
97.420705	3163.182390	22.822106
97.967647	3165.479761	22.827123
98.098238	3163.439399	22.832141
98.211163	3168.222574	22.837159
98.216363	3169.332345	22.842176
98.013584	3170.928436	22.847194
98.471157	3163.124800	22.852211
98.404251	3166.109410	22.857229
98.528967	3154.462497	22.862247
98.624320	3146.141973	22.867264
98.247023	3163.256878	22.872282
98.285292	3153.831256	22.877299
98.267383	3144.963327	22.882317
98.513499	3168.282468	22.887335
98.738813	3182.912865	22.892352
98.547580	3191.584362	22.897370
98.786693	3193.126333	22.902387
98.957620	3199.535703	22.907405
99.016585	3213.002712	22.912423
99.433640	3199.422876	22.917440
99.019552	3214.680595	22.922458
99.378767	3212.630399	22.927475
99.515117	3229.148707	22.932493
99.763209	3242.456147	22.937511
99.919215	3246.425954	22.942528
99.511550	3251.153057	22.947546
100.136111	3243.713901	22.952563
100.073180	3250.886717	22.957581
100.139098	3251.743161	22.962599
100.412721	3264.503899	22.967616
100.359968	3267.263756	22.972634
100.788751	3273.094738	22.977651
100.695055	3278.055786	22.982669
100.573025	3273.454866	22.987687
100.685984	3283.932394	22.992704
100.451408	3285.834135	22.997722
101.078245	3295.535438	23.002739
100.995779	3312.520688	23.007757
101.074196	3310.715300	23.012775
101.738299	3302.408976	23.017792
101.422243	3309.373259	23.022810
101.653541	3296.914554	23.027827
101.740155	3302.633982	23.032845
101.557925	3307.232908	23.037863
102.118023	3311.477682	23.042880
101.788566	3327.417177	23.047898
102.008419	3327.830877	23.052915
101.996967	3327.208811	23.057933
101.864982	3330.349478	23.062951
102.101657	3321.710634	23.067968
102.245210	3334.021674	23.072986
102.524956	3346.603914	23.078003
102.871864	3357.627858	23.083021
102.987417	3353.806534	23.088039
102.921913	3348.759648	23.093056
103.237122	3345.904916	23.098074
103.384921	3350.029252	23.103091
103.222521	3349.789205	23.108109
103.138064	3347.293027	23.113127
103.511626	3346.971897	23.118144
103.603789	3348.275181	23.123162
103.616705	3341.524435	23.128179
103.360105	3355.728341	23.133197
103.450913	3372.327947	23.138215
104.017131	3366.988877	23.143232
103.842776	3373.056172	23.148250
103.833655	3374.325014	23.153267
103.955177	3389.543216	23.158285
104.364506	3400.930885	23.163303
104.632776	3401.707839	23.168320
104.243546	3393.162931	23.173338
104.710179	3386.338375	23.178355
104.657355	3401.489731	23.183373
104.930739	3411.272347	23.188391
105.034012	3420.314982	23.193408
105.083163	3416.103442	23.198426
105.391416	3423.636254	23.203443
105.300077	3430.128034	23.208461
104.894201	3425.102721	23.213479
105.229350	3430.336255	23.218496
105.496524	3431.020874	23.223514
105.557904	3443.225504	23.228531
105.350949	3461.345640	23.233549
105.680250	3459.644839	23.238567
106.003492	3456.754115	23.243584
105.911358	3471.790778	23.248602
106.254256	3473.423500	23.253619
106.550968	3473.712302	23.258637
106.991382	3484.922458	23.263655
107.020457	3472.995839	23.268672
107.151547	3472.762804	23.273690
106.985591	3473.756787	23.278707
107.359588	3468.802984	23.283725
106.782982	3476.090704	23.288743
107.401665	3467.227635	23.293760
107.277054	3477.539435	23.298778
107.363161	3470.948190	23.303795
107.320964	3465.848596	23.308813
107.228636	3473.359831	23.313831
107.314576	3478.828653	23.318848
107.229137	3496.485451	23.323866
107.639452	3500.008189	23.328883
107.608163	3508.060134	23.333901
107.673683	3517.024814	23.338919
107.936583	3523.073457	23.343936
107.681849	3532.526099	23.348954
108.003977	3536.114991	23.353971
108.253310	3538.466716	23.358989
108.154386	3554.057330	23.364007
108.546284	3563.309834	23.369024
108.663845	3575.119855	23.374042
108.483571	3568.766284	23.379059
108.976189	3579.230882	23.384077
108.746549	3591.826627	23.389095
109.482533	3572.945388	23.394112
109.331204	3584.964020	23.399130
109.177096	3581.087200	23.404147
109.437348	3571.525432	23.409165
109.368322	3592.076448	23.414183
109.747098	3593.451289	23.419200
109.861972	3606.780662	23.424218
110.032545	3607.681251	23.429235
110.263624	3591.742846	23.434253
110.402131	3598.944348	23.439271
110.475730	3601.095595	23.444288
110.474502	3597.266343	23.449306
110.795373	3599.896018	23.454323
110.846893	3599.279283	23.459341
110.785444	3598.774127	23.464359
111.071463	3603.949698	23.469376
110.646217	3607.029432	23.474394
111.083900	3620.798386	23.479411
111.136185	3620.298846	23.484429
111.142423	3634.517054	23.489447
111.101252	3619.882655	23.494464
111.516091	3633.002251	23.499482
111.527746	3655.129379	23.504499
112.122943	3665.921966	23.509517
111.679678	3656.248838	23.514535
111.931035	3652.670747	23.519552
111.913711	3654.719704	23.524570
111.709381	3658.481050	23.529587
112.035676	3671.405073	23.534605
112.115842	3684.509541	23.539623
112.531875	3693.590026	23.544640
112.581530	3684.629128	23.549658
112.436272	3712.814928	23.554675
112.947615	3704.022612	23.559693
113.284204	3708.215848	23.564711
113.341108	3707.579715	23.569728
113.484681	3717.003660	23.574746
113.135738	3716.159785	23.579763
113.184520	3706.608469	23.584781
113.246734	3716.915541	23.589799
113.577816	3723.230556	23.594816
113.897490	3728.799820	23.599834
113.838987	3747.446153	23.604851
114.245895	3732.222253	23.609869
113.744646	3738.590162	23.614887
114.259067	3744.287095	23.619904
114.349148	3761.838420	23.624922
114.285788	3764.547361	23.629939
114.363020	3761.833453	23.634957
114.414537	3765.850187	23.639975
114.555181	3769.181721	23.644992
115.103941	3788.276973	23.650010
114.641407	3793.585747	23.655027
115.056633	3782.675403	23.660045
114.879104	3796.724518	23.665063
115.108338	3800.184728	23.670080
115.574731	3816.107784	23.675098
115.243251	3826.457541	23.680115
115.809721	3807.712298	23.685133
115.595730	3825.784809	23.690151
116.009080	3830.965007	23.695168
116.206047	3830.978958	23.700186
115.820187	3841.062906	23.705203
116.026861	3843.920943	23.710221
115.944262	3847.057097	23.715239
116.320500	3850.225308	23.720256
116.544266	3856.388817	23.725274
116.824180	3861.413514	23.730291
117.268565	3863.297228	23.735309
117.264714	3869.665285	23.740327
117.035657	3867.638589	23.745344
117.163489	3862.300925	23.750362
117.242158	3868.741567	23.755379
117.388341	3864.481588	23.760397
117.339506	3868.637767	23.765415
117.476094	3878.118082	23.770432
117.729992	3892.086546	23.775450
117.268788	3902.389678	23.780467
117.628036	3893.008996	23.785485
117.822083	3916.597713	23.790503
118.380576	3922.400029	23.795520
118.330069	3925.897042	23.800538
118.653784	3937.644928	23.805555
118.588614	3932.721026	23.810573
118.599767	3931.355427	23.815591
118.646923	3935.917421	23.820608
119.346713	3946.091733	23.825626
119.371664	3949.351870	23.830643
119.575001	3927.432190	23.835661
119.674465	3945.771159	23.840679
119.655187	3948.865767	23.845696
119.894218	3941.481721	23.850714
119.959001	3953.646031	23.855731
119.998850	3938.961723	23.860749
119.812299	3941.459552	23.865767
120.147743	3946.930225	23.870784
120.125352	3941.975630	23.875802
120.229138	3956.320142	23.880819
120.283444	3961.060098	23.885837
119.813135	3975.095154	23.890855
120.290113	3962.234686	23.895872
120.331004	3974.695092	23.900890
120.257883	3993.626423	23.905907
120.786952	4007.798346	23.910925
120.851803	4012.678704	23.915943
120.884139	4029.324896	23.920960
121.438493	4026.412022	23.925978
121.258432	4025.298487	23.930995
121.524152	4040.352553	23.936013
121.812583	4052.273289	23.941031
121.730997	4051.634829	23.946048
121.962611	4054.057279	23.951066
122.005306	4053.571121	23.956083
122.515364	4049.962005	23.961101
122.543181	4064.358540	23.966119
122.561045	4069.740786	23.971136
122.704770	4071.286797	23.976154
122.742957	4071.568724	23.981171
123.091236	4064.462637	23.986189
123.072475	4073.315971	23.991207
122.857680	4078.070901	23.996224
123.125449	4062.736202	24.001242
123.279486	4088.073560	24.006259
123.518062	4109.951237	24.011277
123.553002	4092.652570	24.016295
123.658437	4101.629890	24.021312
123.839371	4093.714020	24.026330
123.912078	4103.927881	24.031347
124.117505	4120.340052	24.036365
123.911464	4134.010708	24.041383
123.613621	4124.647123	24.046400
124.154809	4138.186832	24.051418
124.369194	4146.771363	24.056435
124.230276	4163.742066	24.061453
124.580914	4171.259185	24.066471
124.567603	4159.087462	24.071488
124.805493	4154.240976	24.076506
124.847478	4181.800605	24.081523
125.388287	4180.601803	24.086541
125.279185	4198.991282	24.091559
125.270137	4190.573668	24.096576
125.487936	4185.849393	24.101594
125.803733	4208.180209	24.106611
125.728298	4210.187658	24.111629
126.073308	4220.491250	24.116647
125.778712	4221.201408	24.121664
126.415314	4211.466035	24.126682
126.698675	4223.421600	24.131699
126.997501	4240.669673	24.136717
127.499493	4231.909711	24.141735
127.255070	4230.801284	24.146752
127.294844	4206.817226	24.151770
127.037827	4197.342910	24.156787
127.147798	4216.686005	24.161805
127.761892	4218.080684	24.166823
127.697289	4222.504925	24.171840
127.452890	4227.583700	24.176858
127.565034	4223.207197	24.181875
127.232447	4224.506328	24.186893
127.692998	4239.600050	24.191911
127.959096	4241.170348	24.196928
127.902718	4256.590456	24.201946
128.046946	4259.935284	24.206963
128.284083	4279.056649	24.211981
128.909816	4282.610905	24.216999
128.528716	4290.067096	24.222016
128.728242	4276.173044	24.227034
128.678465	4282.707919	24.232051
129.014009	4304.650165	24.237069
129.666139	4308.587875	24.242087
129.559047	4311.800613	24.247104
129.456506	4310.670704	24.252122
129.586306	4315.770749	24.257139
129.554230	4311.125522	24.262157
129.763835	4328.080943	24.267175
130.025588	4334.643894	24.272192
130.492568	4343.838002	24.277210
130.324776	4347.099361	24.282227
130.406452	4336.706363	24.287245
130.660585	4342.529209	24.292263
130.504226	4344.427208	24.297280
130.724370	4342.542768	24.302298
130.926514	4361.069993	24.307315
130.807059	4356.842356	24.312333
131.374025	4349.073208	24.317351
131.457233	4348.648460	24.322368
131.394566	4365.457959	24.327386
131.699395	4381.442941	24.332403
131.781611	4381.084107	24.337421
131.948080	4381.854312	24.342439
131.916806	4391.792224	24.347456
132.220637	4371.309708	24.352474
132.157034	4387.941032	24.357491
132.029978	4404.324974	24.362509
132.419029	4406.008836	24.367527
132.220555	4417.933533	24.372544
132.565723	4423.390170	24.377562
132.506411	4433.838670	24.382579
132.723768	4431.872787	24.387597
132.648146	4442.298002	24.392615
132.587716	4454.281810	24.397632
133.232070	4464.914860	24.402650
133.306220	4483.321641	24.407667
132.657179	4482.452502	24.412685
133.222022	4487.325593	24.417703
133.619471	4509.642563	24.422720
133.642514	4513.563403	24.427738
134.073302	4527.020903	24.432755
133.859385	4541.276711	24.437773
134.446482	4529.353539	24.442791
134.350255	4535.091428	24.447808
134.720017	4552.442700	24.452826
134.845788	4562.377607	24.457843
134.819470	4557.145102	24.462861
134.969598	4569.272956	24.467879
135.176620	4574.193782	24.472896
135.215940	4584.412294	24.477914
135.228805	4589.232128	24.482931
135.740663	4587.424662	24.487949
135.862933	4581.597881	24.492967
136.022827	4598.559843	24.497984
136.138705	4607.844014	24.503002
136.485916	4603.037204	24.508019
136.231906	4619.945920	24.513037
136.364312	4618.231466	24.518055
136.506635	4612.345058	24.523072
136.706260	4631.189574	24.528090
136.673711	4639.865577	24.533107
136.910269	4644.563815	24.538125
137.461508	4645.653943	24.543143
137.404766	4639.598043	24.548160
137.386889	4652.217923	24.553178
137.724702	4676.175398	24.558195
137.725278	4672.964125	24.563213
137.693679	4668.869927	24.568231
137.312417	4677.020857	24.573248
137.811392	4691.709435	24.578266
138.097623	4692.325213	24.583283
137.891642	4713.859059	24.588301
138.728748	4716.706009	24.593319
138.857209	4729.113175	24.598336
139.040933	4724.655803	24.603354
139.490905	4720.078449	24.608371
139.172621	4709.565453	24.613389
139.401865	4715.615400	24.618407
139.645122	4716.872179	24.623424
139.741147	4723.683953	24.628442
139.923477	4743.523652	24.633459
140.194627	4759.812639	24.638477
140.269482	4742.844868	24.643495
140.234044	4739.938764	24.648512
140.333458	4749.277319	24.653530
140.467566	4751.374237	24.658547
140.263563	4749.159807	24.663565
140.216828	4744.538133	24.668583
140.501026	4786.063666	24.673600
140.453069	4789.677782	24.678618
141.084214	4786.857602	24.683635
140.820744	4790.479374	24.688653
141.341517	4800.085760	24.693671
141.270324	4806.188930	24.698688
141.170587	4816.758546	24.703706
141.674202	4829.702271	24.708723
141.578991	4844.266323	24.713741
141.681820	4843.006764	24.718759
141.779376	4867.131801	24.723776
141.784449	4863.010230	24.728794
142.113996	4875.887080	24.733811
142.176856	4892.895319	24.738829
142.423035	4885.261597	24.743847
142.849143	4898.183932	24.748864
142.873795	4898.870896	24.753882
143.082874	4901.327522	24.758899
142.956698	4924.665537	24.763917
143.168932	4923.459947	24.768935
143.307110	4932.798507	24.773952
143.724284	4948.727710	24.778970
143.735386	4945.846164	24.783987
143.728808	4955.070062	24.789005
144.133321	4948.370065	24.794023
144.106176	4972.796994	24.799040
144.080433	4971.796877	24.804058
144.408624	4975.405187	24.809075
144.602880	4994.738864	24.814093
144.919883	4989.922753	24.819111
145.276116	5007.381500	24.824128
145.211040	5006.607584	24.829146
145.772605	5006.299069	24.834163
145.441735	5015.635253	24.839181
145.880157	5004.326102	24.844199
146.096110	5012.812419	24.849216
146.105749	5027.628630	24.854234
146.307079	5029.862522	24.859251
146.211927	5029.014040	24.864269
146.731384	5029.627126	24.869287
146.474332	5029.098727	24.874304
146.589932	5036.581475	24.879322
146.590112	5053.599853	24.884339
146.461490	5069.787883	24.889357
146.952344	5058.519639	24.894375
146.916410	5060.034014	24.899392
147.165498	5079.124463	24.904410
147.620188	5086.265355	24.909427
147.396762	5089.048616	24.914445
147.382892	5109.161377	24.919463
147.812729	5113.580556	24.924480
147.676617	5121.483710	24.929498
147.926864	5131.957911	24.934515
148.196467	5143.749120	24.939533
148.430407	5145.256709	24.944551
148.474306	5161.151343	24.949568
149.190888	5180.546989	24.954586
149.174920	5179.579106	24.959603
149.204379	5183.517953	24.964621
149.266091	5171.944518	24.969639
149.388294	5188.897206	24.974656
149.700915	5208.770305	24.979674
150.037235	5201.992484	24.984691
149.827349	5215.697006	24.989709
149.953612	5210.858403	24.994727
150.308673	5214.629667	24.999744
149.882021	5236.926748	25.004762
150.430541	5231.987262	25.009779
150.437463	5248.047558	25.014797
150.696475	5243.172835	25.019815
150.835657	5256.268480	25.024832
150.902540	5265.111095	25.029850
151.228678	5257.324598	25.034867
151.535199	5272.718819	25.039885
151.617708	5290.445182	25.044903
151.928774	5291.932561	25.049920
151.861958	5297.621771	25.054938
152.309211	5290.034952	25.059955
152.218806	5292.361186	25.064973
152.097231	5287.012274	25.069991
152.395141	5309.870120	25.075008
152.396209	5308.146581	25.080026
152.473757	5297.798513	25.085043
152.098880	5321.920809	25.090061
152.855996	5338.021036	25.095079
153.439694	5331.188898	25.100096
153.145747	5352.390483	25.105114
153.593027	5350.672747	25.110131
153.611756	5371.509275	25.115149
153.649815	5373.430789	25.120167
153.684450	5373.838143	25.125184
153.832643	5374.720092	25.130202
153.964020	5393.260237	25.135219
154.222839	5399.060657	25.140237
154.314685	5402.163572	25.145255
154.342015	5409.329553	25.150272
154.979072	5434.020722	25.155290
154.743354	5430.834556	25.160307
155.271997	5431.615846	25.165325
155.125691	5447.135855	25.170343
155.776816	5466.477706	25.175360
155.846485	5459.131562	25.180378
155.969339	5457.550107	25.185395
156.117928	5464.698439	25.190413
156.392183	5461.800091	25.195431
156.730688	5475.991458	25.200448
156.342371	5486.945467	25.205466
156.435917	5483.165061	25.210483
156.321911	5483.739907	25.215501
156.973651	5498.167365	25.220519
156.869977	5497.291915	25.225536
157.401283	5511.605412	25.230554
157.659983	5505.624235	25.235571
157.710998	5511.858684	25.240589
157.789636	5520.771557	25.245607
158.177326	5526.204628	25.250624
158.102982	5536.432699	25.255642
158.383032	5530.665333	25.260659
158.226998	5540.330460	25.265677
158.314459	5550.079785	25.270695
158.657231	5550.631133	25.275712
158.363587	5560.825370	25.280730
158.395751	5562.584083	25.285747
158.334390	5589.372235	25.290765
158.680116	5599.811680	25.295783
159.635216	5620.040223	25.300800
159.431250	5625.077329	25.305818
159.896018	5631.204479	25.310835
160.098060	5643.239147	25.315853
159.973041	5658.422342	25.320871
160.381515	5658.069421	25.325888
160.350133	5667.844755	25.330906
160.516382	5646.485951	25.335923
160.935721	5677.077587	25.340941
161.334298	5689.329848	25.345959
161.374214	5686.048079	25.350976
161.408626	5680.091295	25.355994
161.864533	5683.691269	25.361011
161.620690	5685.298726	25.366029
161.736077	5686.577501	25.371047
162.037813	5696.482875	25.376064
161.624693	5707.969155	25.381082
162.131538	5706.856184	25.386099
161.822217	5711.425624	25.391117
162.178154	5727.634675	25.396135
162.434717	5744.374009	25.401152
162.363642	5755.232867	25.406170
162.667431	5754.846842	25.411187
162.738502	5770.600579	25.416205
163.112342	5790.171744	25.421223
163.756890	5788.402073	25.426240
163.618807	5802.626022	25.431258
163.675164	5787.680129	25.436275
163.800387	5787.785086	25.441293
163.851110	5808.192443	25.446311
163.850313	5816.159033	25.451328
164.065398	5825.038902	25.456346
164.342996	5843.432175	25.461363
164.560270	5859.370927	25.466381
164.435377	5852.970257	25.471399
164.687386	5864.165230	25.476416
164.691947	5883.167914	25.481434
165.166456	5894.191087	25.486451
165.297315	5904.433136	25.491469
165.714173	5925.555060	25.496487
166.088682	5925.288861	25.501504
165.882062	5929.227922	25.506522
166.348965	5937.894176	25.511539
166.422345	5955.098710	25.516557
166.214661	5946.444035	25.521575
167.280302	5954.080134	25.526592
166.950387	5965.896209	25.531610
167.391859	5975.428621	25.536627
167.534857	5965.047248	25.541645
167.547411	5968.906004	25.546663
167.533669	5972.863214	25.551680
167.676609	5988.745473	25.556698
167.834944	6009.076247	25.561715
168.103792	6004.663119	25.566733
168.066729	6003.411620	25.571751
168.553486	6022.229666	25.576768
168.181655	6043.120200	25.581786
168.492048	6038.650190	25.586803
168.660395	6042.695458	25.591821
168.844402	6064.675457	25.596839
169.180233	6068.752123	25.601856
168.905808	6079.647167	25.606874
169.597924	6104.803600	25.611891
169.325166	6102.798004	25.616909
169.238180	6122.914697	25.621927
169.718822	6127.539192	25.626944
169.861011	6156.215445	25.631962
169.966082	6161.322544	25.636979
170.531843	6182.235537	25.641997
170.817340	6201.448133	25.647015
171.096784	6181.146054	25.652032
170.912994	6194.858930	25.657050
171.072701	6208.487498	25.662067
171.649044	6211.139990	25.667085
171.610931	6223.289206	25.672103
171.805334	6222.338869	25.677120
171.623110	6234.635547	25.682138
172.132660	6255.968229	25.687156
172.286931	6250.378889	25.692173
172.350242	6278.535242	25.697191
172.255572	6271.185946	25.702208
172.547911	6284.824955	25.707226
172.614621	6296.018171	25.712244
173.192597	6299.237431	25.717261
173.067875	6322.417022	25.722279
173.264410	6325.740265	25.727296
173.491745	6342.257470	25.732314
173.756475	6353.994483	25.737332
174.136432	6358.590794	25.742349
173.780544	6365.043628	25.747367
174.403120	6379.388913	25.752384
174.433552	6390.639380	25.757402
174.850582	6390.785513	25.762420
174.840474	6390.512374	25.767437
174.595432	6404.601757	25.772455
175.564876	6414.570912	25.777472
175.323956	6424.489625	25.782490
175.373211	6423.821571	25.787508
175.552794	6429.689808	25.792525
175.429149	6461.611096	25.797543
175.997265	6459.671275	25.802560
176.164154	6468.490957	25.807578
175.857376	6488.004163	25.812596
176.342373	6489.091991	25.817613
176.057853	6509.838772	25.822631
176.421316	6520.757879	25.827648
176.893727	6533.416001	25.832666
177.168254	6552.026006	25.837684
177.519713	6548.093261	25.842701
177.945743	6568.455738	25.847719
178.133516	6572.774363	25.852736
178.355713	6581.601508	25.857754
178.634512	6572.512105	25.862772
178.987287	6568.985510	25.867789
178.679703	6568.960769	25.872807
179.150243	6576.322210	25.877824
179.164093	6591.149441	25.882842
179.253601	6597.654784	25.887860
179.490542	6602.504762	25.892877
179.159524	6600.630008	25.897895
179.789335	6617.451936	25.902912
180.000146	6637.469679	25.907930
180.142177	6633.357304	25.912948
180.467705	6631.689873	25.917965
180.366326	6660.677421	25.922983
180.451915	6664.663282	25.928000
180.436965	6657.199040	25.933018
180.627275	6676.992618	25.938036
181.196944	6671.928307	25.943053
181.162310	6690.458038	25.948071
181.413949	6706.243913	25.953088
181.648438	6726.465771	25.958106
181.574274	6721.083333	25.963124
181.902249	6741.252747	25.968141
181.796708	6755.952587	25.973159
182.006812	6754.857865	25.978176
182.485339	6781.738406	25.983194
182.467237	6787.032235	25.988212
182.823179	6796.598182	25.993229
182.960330	6819.836831	25.998247
183.218665	6819.256286	26.003264
183.122474	6827.451790	26.008282
183.115609	6847.007242	26.013300
183.596293	6866.634160	26.018317
183.747451	6879.028255	26.023335
183.938791	6880.983695	26.028352
184.311978	6908.006292	26.033370
184.529125	6902.629212	26.038388
184.904969	6909.344119	26.043405
184.909689	6925.713643	26.048423
184.991916	6922.026120	26.053440
185.434546	6924.929224	26.058458
185.472203	6958.282644	26.063476
186.070506	6952.640954	26.068493
186.074203	6965.132724	26.073511
186.186198	6962.797246	26.078528
186.392842	6977.168488	26.083546
186.376984	6997.419457	26.088564
186.654293	6993.800492	26.093581
186.832683	7007.560554	26.098599
186.697158	7011.015202	26.103616
186.852460	7012.026808	26.108634
187.026193	7025.659281	26.113652
187.380326	7041.014298	26.118669
187.605621	7054.906838	26.123687
187.819402	7067.565596	26.128704
188.115004	7068.161814	26.133722
187.857825	7097.260177	26.138740
188.331260	7093.091350	26.143757
188.200473	7107.884684	26.148775
188.880908	7121.969068	26.153792
188.677127	7125.234976	26.158810
188.597794	7139.332287	26.163828
189.137080	7137.879147	26.168845
189.336018	7167.125946	26.173863
189.626919	7200.708961	26.178880
190.077212	7193.298331	26.183898
189.836703	7201.444630	26.188916
190.312306	7206.611346	26.193933
190.167599	7216.631220	26.198951
190.426512	7242.331241	26.203968
190.872217	7241.874876	26.208986
190.789010	7254.017373	26.214004
190.952018	7267.465172	26.219021
191.453700	7288.198847	26.224039
191.600126	7301.547816	26.229056
191.973341	7310.833208	26.234074
192.162244	7320.168748	26.239092
192.587863	7329.399024	26.244109
192.024337	7340.532510	26.249127
192.267760	7341.972987	26.254144
192.837761	7357.539160	26.259162
192.876857	7370.356976	26.264180
193.139866	7375.968419	26.269197
193.016680	7388.976880	26.274215
193.414623	7400.713143	26.279232
193.886513	7413.595737	26.284250
194.327684	7435.189411	26.289268
194.328013	7424.369519	26.294285
194.561890	7437.725420	26.299303
194.408229	7445.501504	26.304320
195.131526	7458.380400	26.309338
194.737264	7461.447086	26.314356
195.276709	7474.631241	26.319373
195.414138	7487.727463	26.324391
195.715371	7503.279906	26.329408
195.942322	7504.463215	26.334426
196.047394	7518.532759	26.339444
196.187286	7514.168479	26.344461
196.390062	7535.697718	26.349479
196.610157	7551.740109	26.354496
197.027078	7547.666350	26.359514
196.828537	7562.135002	26.364532
197.204521	7580.175782	26.369549
197.313555	7592.554558	26.374567
197.578901	7583.621167	26.379584
197.868717	7610.888723	26.384602
197.738100	7632.119547	26.389620
197.884418	7617.702073	26.394637
198.292098	7627.953852	26.399655
198.726990	7648.862072	26.404672
198.522545	7659.661579	26.409690
198.525831	7678.524871	26.414708
199.237670	7669.837425	26.419725
199.150418	7689.061446	26.424743
199.361829	7712.679791	26.429760
200.039302	7707.695005	26.434778
199.759010	7710.800402	26.439796
200.134946	7728.126217	26.444813
200.377337	7743.921750	26.449831
200.301405	7744.875523	26.454848
200.783721	7743.907456	26.459866
200.714778	7761.731332	26.464884
200.672203	7779.036565	26.469901
200.780627	7785.159648	26.474919
200.976180	7796.249156	26.479936
201.454597	7809.334199	26.484954
201.384114	7838.270759	26.489972
201.705440	7832.496526	26.494989
202.191067	7860.364609	26.500007
202.248436	7862.261972	26.505024
202.599594	7887.762716	26.510042
202.331208	7899.325118	26.515060
202.885743	7911.717174	26.520077
203.219849	7923.941668	26.525095
203.110208	7933.021305	26.530112
203.342125	7950.802772	26.535130
203.561012	7954.959902	26.540148
203.708054	7984.316028	26.545165
204.400585	7992.783503	26.550183
204.777992	7994.964316	26.555200
205.079839	8010.569928	26.560218
205.327218	8036.859924	26.565236
205.500403	8016.389532	26.570253
205.733386	8028.251972	26.575271
205.099621	8034.940421	26.580288
205.562191	8054.172492	26.585306
205.720522	8056.049260	26.590324
206.123002	8063.032778	26.595341
206.476189	8082.439693	26.600359
206.661109	8099.591120	26.605376
206.960908	8111.918306	26.610394
206.756825	8117.684377	26.615412
206.846175	8120.144363	26.620429
207.157820	8132.405023	26.625447
207.044760	8154.963941	26.630464
207.425379	8170.488173	26.635482
207.800491	8197.392156	26.640500
208.469678	8202.776896	26.645517
208.447576	8209.179264	26.650535
208.212907	8242.285028	26.655552
208.823322	8236.457372	26.660570
208.964018	8264.739168	26.665588
209.276251	8275.476567	26.670605
209.415550	8277.777100	26.675623
209.477063	8301.818844	26.680640
210.068357	8324.170261	26.685658
210.161457	8324.942552	26.690676
210.856950	8321.299877	26.695693
211.125731	8332.260305	26.700711
211.168844	8335.805446	26.705728
211.462119	8348.770302	26.710746
211.287284	8355.716226	26.715764
211.674409	8355.649942	26.720781
211.736707	8364.933769	26.725799
211.670994	8383.446990	26.730816
212.132606	8383.882724	26.735834
211.752051	8402.202244	26.740852
212.314514	8412.048533	26.745869
212.368900	8421.825974	26.750887
212.202198	8443.908981	26.755904
212.806089	8459.642351	26.760922
212.942161	8484.718039	26.765940
212.897177	8506.948003	26.770957
213.168260	8510.593353	26.775975
213.159035	8532.607932	26.780992
214.030439	8556.710798	26.786010
213.978489	8574.167312	26.791028
214.403162	8591.463969	26.796045
214.317251	8588.687577	26.801063
214.649620	8600.706520	26.806080
215.279078	8610.128350	26.811098
215.855594	8616.583992	26.816116
215.769640	8626.324885	26.821133
216.230130	8629.755447	26.826151
215.979261	8635.501079	26.831168
216.350057	8643.906281	26.836186
216.568046	8648.652904	26.841204
216.510020	8663.977570	26.846221
216.868110	8677.745629	26.851239
216.880919	8698.150779	26.856256
217.620600	8700.246632	26.861274
217.612594	8713.389165	26.866292
217.263562	8730.390839	26.871309
217.946449	8726.414618	26.876327
218.269419	8758.751943	26.881344
218.370596	8763.898337	26.886362
218.679635	8763.696876	26.891380
218.887997	8785.588426	26.896397
218.989702	8798.556160	26.901415
219.237752	8809.652671	26.906432
219.234302	8814.775410	26.911450
219.655402	8841.178241	26.916468
219.748136	8859.437416	26.921485
220.083920	8854.961639	26.926503
220.168293	8883.494080	26.931520
220.582536	8891.389708	26.936538
220.598110	8917.984119	26.941556
220.743734	8934.983836	26.946573
221.066830	8945.265415	26.951591
221.085581	8961.137711	26.956608
221.364741	8983.701528	26.961626
221.539421	9000.907610	26.966644
221.588905	9020.510785	26.971661
222.106173	9030.387771	26.976679
222.278986	9057.767733	26.981696
222.445892	9072.063954	26.986714
223.172755	9092.981769	26.991732
223.261605	9118.406533	26.996749
223.878621	9118.786684	27.001767
223.595963	9126.535280	27.006784
223.889088	9152.376895	27.011802
224.201129	9165.047093	27.016820
224.220726	9182.193138	27.021837
224.588745	9193.237801	27.026855
224.269006	9211.181932	27.031872
225.043412	9225.382645	27.036890
225.195469	9248.131675	27.041908
225.017197	9266.170647	27.046925
225.432089	9283.161693	27.051943
225.649595	9301.272369	27.056960
225.955682	9308.916690	27.061978
226.722881	9329.738358	27.066996
226.515100	9336.918580	27.072013
226.940746	9353.429802	27.077031
226.875722	9364.344486	27.082048
227.236019	9385.981757	27.087066
227.669320	9395.208039	27.092084
227.497586	9415.791898	27.097101
227.949840	9424.566085	27.102119
227.870328	9436.992420	27.107136
227.987031	9461.734931	27.112154
228.127786	9476.543896	27.117172
228.368423	9505.599865	27.122189
229.140112	9508.297853	27.127207
229.132141	9542.466118	27.132224
229.271245	9543.649133	27.137242
229.244001	9553.206812	27.142260
229.731373	9576.323114	27.147277
230.076533	9597.111675	27.152295
230.013353	9610.978505	27.157312
230.215021	9633.615913	27.162330
230.900579	9640.362739	27.167348
230.620176	9666.392897	27.172365
231.044764	9672.227376	27.177383
230.966463	9698.146212	27.182400
231.548831	9713.544101	27.187418
231.759095	9726.512772	27.192436
231.847814	9753.581717	27.197453
232.414437	9753.239226	27.202471
232.855678	9777.441807	27.207488
232.970936	9783.622824	27.212506
233.653519	9807.190860	27.217524
233.749387	9814.326640	27.222541
233.989032	9812.005103	27.227559
234.504890	9830.465667	27.232576
234.770327	9837.130751	27.237594
234.693381	9849.816927	27.242612
234.809597	9860.935167	27.247629
235.312013	9860.164530	27.252647
235.363246	9871.696821	27.257664
235.255524	9895.882366	27.262682
235.470595	9901.894910	27.267700
235.599983	9919.404071	27.272717
235.884649	9940.370859	27.277735
236.231279	9962.786282	27.282752
236.391415	9988.160482	27.287770
236.676946	9992.808913	27.292788
236.658820	10013.620231	27.297805
237.080353	10020.595169	27.302823
237.147463	10050.867891	27.307840
237.364020	10076.669306	27.312858
237.680908	10071.496032	27.317876
237.736495	10103.419452	27.322893
238.022738	10135.575803	27.327911
238.196799	10146.083653	27.332928
238.209794	10176.590055	27.337946
238.801324	10202.417157	27.342964
239.244950	10222.234756	27.347981
239.234689	10223.464557	27.352999
239.847552	10244.761143	27.358016
240.036252	10265.028958	27.363034
240.374935	10288.319741	27.368052
240.581561	10302.986251	27.373069
241.014170	10304.850269	27.378087
241.164252	10331.573695	27.383104
241.289709	10348.658602	27.388122
241.892576	10348.862314	27.393140
241.717354	10389.562755	27.398157
242.021016	10388.950970	27.403175
242.586929	10402.352190	27.408192
242.386858	10418.581909	27.413210
242.708527	10431.089253	27.418228
242.761752	10445.515772	27.423245
243.397859	10455.408676	27.428263
243.892257	10469.860006	27.433280
244.049345	10473.516769	27.438298
244.306499	10494.832286	27.443316
244.226895	10516.170384	27.448333
244.945244	10521.550957	27.453351
244.845073	10543.070518	27.458368
244.674102	10557.523151	27.463386
245.119857	10558.171117	27.468404
245.074577	10584.033154	27.473421
245.446650	10599.068837	27.478439
245.728796	10620.208663	27.483456
245.605893	10639.120733	27.488474
246.185374	10649.071954	27.493492
245.957446	10680.513214	27.498509
246.299614	10697.265707	27.503527
246.619408	10727.319142	27.508544
246.973506	10737.815755	27.513562
247.389578	10747.356046	27.518580
247.541604	10788.710046	27.523597
248.103356	10798.703678	27.528615
248.147828	10810.585162	27.533632
248.003116	10831.718593	27.538650
248.334026	10847.809814	27.543668
248.355866	10878.013592	27.548685
248.953920	10898.643905	27.553703
249.595088	10925.816561	27.558720
249.388681	10944.767208	27.563738
249.641230	10970.197021	27.568756
249.839847	10995.100894	27.573773
250.626661	10998.511938	27.578791
250.851763	11028.322409	27.583808
250.994657	11044.072278	27.588826
251.247227	11072.350025	27.593844
251.526590	11089.897924	27.598861
251.749159	11099.114324	27.603879
251.986779	11109.961290	27.608896
251.984799	11139.525888	27.613914
252.812863	11146.887124	27.618932
253.099932	11172.087040	27.623949
253.074594	11189.292291	27.628967
253.607186	11207.883245	27.633984
253.346712	11225.860013	27.639002
253.858316	11236.646830	27.644020
254.487911	11265.254940	27.649037
254.720559	11268.629982	27.654055
254.857951	11276.591449	27.659072
255.209016	11298.098917	27.664090
255.570387	11297.124642	27.669108
255.909955	11333.979208	27.674125
255.822345	11342.207913	27.679143
256.272876	11331.990842	27.684160
256.107282	11365.588752	27.689178
256.581708	11362.449877	27.694196
256.667939	11378.779003	27.699213
256.869821	11405.137220	27.704231
257.178188	11430.497883	27.709248
257.552712	11452.082824	27.714266
257.870893	11470.081642	27.719284
257.820545	11483.337436	27.724301
258.019335	11503.523222	27.729319
258.242615	11524.291890	27.734336
258.319957	11551.217649	27.739354
258.904314	11577.005620	27.744372
259.045066	11589.144350	27.749389
259.144318	11607.147981	27.754407
259.715087	11635.482866	27.759424
259.600171	11652.979928	27.764442
259.641755	11686.332362	27.769460
260.325125	11711.434562	27.774477
260.483490	11728.032582	27.779495
261.344183	11735.691218	27.784512
261.449808	11771.829939	27.789530
261.976451	11773.284699	27.794548
261.835670	11787.806714	27.799565
262.057821	11811.412818	27.804583
262.388970	11820.158708	27.809600
262.776967	11830.132851	27.814618
262.953371	11855.816930	27.819636
263.201771	11872.236360	27.824653
263.304095	11878.083931	27.829671
263.293201	11894.644699	27.834688
263.457728	11925.708429	27.839706
263.985473	11940.515612	27.844724
264.082674	11960.353211	27.849741
264.193903	11991.998614	27.854759
264.543087	12006.165717	27.859776
264.827303	12036.039983	27.864794
264.956138	12065.923432	27.869812
265.294045	12094.306265	27.874829
265.671017	12116.523525	27.879847
266.091224	12135.523308	27.884864
266.202006	12164.972683	27.889882
266.817563	12181.063909	27.894900
266.852540	12211.973911	27.899917
267.123388	12235.916083	27.904935
267.243829	12243.064643	27.909952
267.390259	12280.473252	27.914970
267.517811	12298.569883	27.919988
268.233476	12329.254203	27.925005
268.380243	12349.063608	27.930023
268.962300	12374.239521	27.935040
269.126318	12390.592275	27.940058
269.464768	12412.415302	27.945076
269.867814	12424.849309	27.950093
270.102585	12456.344432	27.955111
270.577251	12470.790591	27.960128
270.192900	12479.809468	27.965146
270.742376	12510.278149	27.970164
271.106484	12536.355370	27.975181
271.407333	12548.872536	27.980199
271.337805	12562.434129	27.985216
271.581742	12602.086901	27.990234
272.333208	12614.651786	27.995252
272.530663	12639.124296	28.000269
272.892289	12659.862119	28.005287
273.226061	12680.639236	28.010304
273.085294	12698.160610	28.015322
273.582818	12716.320278	28.020340
274.303934	12730.321000	28.025357
274.426769	12754.615354	28.030375
274.632993	12764.847012	28.035392
274.904686	12794.077140	28.040410
275.098940	12807.592994	28.045428
275.462989	12818.918938	28.050445
275.693452	12839.864596	28.055463
276.189676	12862.720255	28.060480
276.159189	12882.294093	28.065498
276.017866	12907.681744	28.070516
276.641226	12930.535403	28.075533
276.904595	12952.418050	28.080551
277.402443	12966.750525	28.085568
277.471883	12991.449563	28.090586
277.398947	13015.281876	28.095604
277.840615	13020.659382	28.100621
278.207226	13046.801620	28.105639
279.042179	13056.226814	28.110656
280.373982	13029.707923	28.115674
280.554791	13033.574865	28.120692
281.306442	13030.267755	28.125709
281.665554	13026.095819	28.130727
281.875012	13018.343349	28.135744
281.870777	13010.118803	28.140762
282.138719	13008.793512	28.145780
282.409028	13001.965401	28.150797
282.183423	12991.963780	28.155815
282.538707	12984.648920	28.160832
282.619292	12987.193044	28.165850
282.556624	12994.029471	28.170868
282.997082	13004.933235	28.175885
282.548576	13013.519440	28.180903
283.021945	13020.721127	28.185920
283.158913	13042.301756	28.190938
283.560269	13065.173377	28.195956
283.619981	13061.329801	28.200973
283.735990	13091.665565	28.205991
284.181911	13108.353013	28.211008
284.034066	13126.841946	28.216026
284.188118	13163.909410	28.221044
285.015986	13189.703072	28.226061
284.881696	13220.877756	28.231079
285.057586	13230.128305	28.236096
285.238142	13274.161170	28.241114
285.685899	13291.108502	28.246132
286.369415	13306.573512	28.251149
286.358282	13342.184314	28.256167
287.008601	13366.261654	28.261184
287.346232	13368.296948	28.266202
287.323191	13416.999723	28.271220
288.088630	13423.997337	28.276237
288.074670	13440.731167	28.281255
288.460849	13446.524533	28.286272
289.093247	13483.230062	28.291290
289.048149	13495.229174	28.296308
289.279041	13510.283821	28.301325
289.670824	13534.585340	28.306343
290.213490	13541.131320	28.311360
290.618483	13569.062873	28.316378
290.625175	13585.813926	28.321396
291.096774	13598.767767	28.326413
291.541180	13611.552774	28.331431
291.754390	13639.824988	28.336448
292.033283	13653.400054	28.341466
292.106863	13681.262067	28.346484
292.029859	13694.478380	28.351501
292.178506	13722.655827	28.356519
292.520931	13745.238746	28.361536
292.802651	13772.103716	28.366554
293.049280	13801.021495	28.371572
293.489011	13814.987712	28.376589
293.622376	13852.265022	28.381607
293.630193	13887.278235	28.386624
294.337768	13905.637761	28.391642
294.023171	13946.902038	28.396660
294.956930	13975.107796	28.401677
295.194253	14003.753281	28.406695
295.670009	14018.895588	28.411712
296.062790	14048.259257	28.416730
296.422567	14079.068739	28.421748
296.868642	14092.383330	28.426765
296.825403	14114.182683	28.431783
297.138701	14132.190010	28.436800
297.649311	14157.631070	28.441818
297.945854	14181.539577	28.446836
298.403293	14208.472365	28.451853
298.249887	14231.695726	28.456871
298.488134	14246.009196	28.461888
298.968101	14272.358458	28.466906
299.284929	14308.188242	28.471924
299.489052	14318.455900	28.476941
299.496181	14355.153244	28.481959
299.728190	14379.721957	28.486976
300.371295	14402.668991	28.491994
300.336295	14429.396696	28.497012
300.987938	14449.795793	28.502029
301.225710	14473.142399	28.507047
301.547897	14499.421969	28.512064
302.011224	14512.976740	28.517082
302.160360	14545.541182	28.522100
302.726041	14563.285094	28.527117
302.923834	14578.998615	28.532135
303.133087	14592.683677	28.537152
303.368703	14628.407817	28.542170
303.551851	14651.294091	28.547188
304.121801	14661.619720	28.552205
304.125074	14691.701320	28.557223
304.536459	14715.114145	28.562240
304.780335	14736.409888	28.567258
305.134549	14774.081468	28.572276
305.332131	14796.667717	28.577293
305.612631	14817.268848	28.582311
305.733871	14843.380457	28.587328
306.518128	14877.271555	28.592346
306.335296	14904.810839	28.597364
307.002294	14929.618972	28.602381
307.409615	14970.383626	28.607399
307.892838	14972.190204	28.612416
308.169512	14999.075373	28.617434
308.151721	15027.682860	28.622452
308.637872	15056.528632	28.627469
308.919532	15082.090913	28.632487
309.585039	15104.062894	28.637504
309.784095	15119.951656	28.642522
310.144660	15144.821775	28.647540
310.656976	15161.990488	28.652557
311.033712	15190.159585	28.657575
311.421058	15202.416307	28.662592
311.651990	15217.140008	28.667610
311.739896	15242.003315	28.672628
312.343526	15251.505844	28.677645
312.130615	15281.636854	28.682663
312.432449	15293.735994	28.687680
312.992452	15320.937353	28.692698
313.057543	15352.253381	28.697716
313.045798	15371.541872	28.702733
313.795643	15398.833346	28.707751
313.791270	15428.997941	28.712768
314.407705	15455.696926	28.717786
314.973912	15472.869672	28.722804
315.343370	15493.709117	28.727821
315.486222	15525.750182	28.732839
315.271847	15555.057705	28.737856
315.875990	15569.554590	28.742874
316.381825	15598.007228	28.747892
316.644864	15625.603294	28.752909
317.211475	15648.407130	28.757927
317.154046	15674.445571	28.762944
317.653212	15703.903396	28.767962
317.753320	15724.344781	28.772980
318.339936	15741.605846	28.777997
318.632561	15760.647514	28.783015
318.392865	15800.034973	28.788032
319.202963	15799.180950	28.793050
319.165707	15850.251036	28.798068
319.281401	15877.912847	28.803085
319.612584	15895.731627	28.808103
320.095724	15917.369202	28.813120
320.995325	15955.380507	28.818138
320.870016	15975.785374	28.823156
321.386322	15990.634413	28.828173
321.663295	16009.273921	28.833191
322.020979	16038.391663	28.838208
322.808982	16031.098522	28.843226
322.810033	16076.052765	28.848244
323.332110	16072.261329	28.853261
323.988288	16083.853351	28.858279
324.034695	16104.981774	28.863296
324.395062	16106.077506	28.868314
324.628248	16139.942495	28.873332
325.091797	16157.733390	28.878349
324.883530	16172.656594	28.883367
325.470288	16191.500449	28.888384
325.652417	16207.024274	28.893402
325.887384	16242.187833	28.898420
326.418605	16258.427870	28.903437
326.515975	16284.304591	28.908455
326.801999	16314.008342	28.913472
326.962452	16325.948784	28.918490
326.862183	16357.937081	28.923508
327.191499	16384.678717	28.928525
327.719688	16424.533412	28.933543
327.831582	16463.394714	28.938560
328.265260	16493.227274	28.943578
328.835801	16521.002579	28.948596
329.410985	16557.883682	28.953613
329.599716	16579.548707	28.958631
329.721792	16611.614242	28.963648
330.235486	16644.683722	28.968666
330.219998	16684.502780	28.973684
330.800321	16705.616270	28.978701
331.390057	16733.401373	28.983719
332.063950	16765.016698	28.988736
332.530066	16788.538512	28.993754
332.803889	16806.708197	28.998772
332.942628	16821.199552	29.003789
333.193243	16840.500015	29.008807
333.659386	16866.064555	29.013824
334.289470	16889.613013	29.018842
334.379776	16912.620238	29.023860
334.820973	16931.886172	29.028877
335.117019	16958.572773	29.033895
334.952977	16988.916344	29.038912
335.335233	17009.449842	29.043930
335.598303	17051.428749	29.048948
336.094338	17076.769599	29.053965
336.655266	17103.174682	29.058983
336.705883	17131.353715	29.064000
337.356138	17160.630014	29.069018
337.341004	17184.893873	29.074036
337.610455	17220.723685	29.079053
338.137918	17236.965315	29.084071
338.244555	17267.666597	29.089088
338.929370	17297.798001	29.094106
339.102144	17340.941570	29.099124
339.176498	17363.195511	29.104141
339.692835	17382.559891	29.109159
339.755838	17424.571226	29.114176
340.170766	17448.028363	29.119194
340.625512	17489.773399	29.124212
340.855948	17522.090754	29.129229
341.460713	17543.618968	29.134247
341.643492	17585.030897	29.139264
341.833676	17605.475505	29.144282
342.459381	17641.141774	29.149300
342.615021	17681.332167	29.154317
343.237950	17706.667211	29.159335
343.485049	17737.073483	29.164352
343.572454	17756.814944	29.169370
344.016544	17785.478605	29.174388
344.270863	17811.338104	29.179405
344.850579	17843.516425	29.184423
345.139902	17862.360902	29.189440
345.613778	17887.925755	29.194458
345.982893	17920.898745	29.199476
346.032548	17956.293607	29.204493
346.399537	17973.315902	29.209511
346.665591	18011.922113	29.214528
347.160423	18023.958289	29.219546
347.679167	18055.374755	29.224564
347.909647	18092.595237	29.229581
348.300452	18102.140899	29.234599
348.509168	18145.175027	29.239616
348.752622	18172.966180	29.244634
349.145709	18204.625937	29.249652
349.592870	18243.839565	29.254669
350.134366	18260.291105	29.259687
350.534962	18293.360518	29.264704
350.935134	18326.754771	29.269722
351.119548	18355.320460	29.274740
351.480471	18384.427638	29.279757
351.618974	18407.931808	29.284775
351.874688	18449.434734	29.289792
352.388563	18478.663402	29.294810
352.416238	18517.004380	29.299828
352.580861	18552.548608	29.304845
353.015102	18577.637166	29.309863
353.174251	18620.198382	29.314880
354.074992	18659.801487	29.319898
354.466125	18689.326651	29.324916
354.668924	18733.348455	29.329933
355.605835	18769.457551	29.334951
355.955790	18796.661546	29.339968
356.455886	18819.461865	29.344986
357.059557	18843.056893	29.350004
357.124142	18863.348840	29.355021
357.833920	18886.622177	29.360039
358.000093	18919.187748	29.365056
358.365555	18928.017710	29.370074
358.748169	18957.522693	29.375092
358.913472	18987.572772	29.380109
359.732030	19017.828673	29.385127
359.483770	19048.379090	29.390144
359.686090	19070.763938	29.395162
359.941892	19105.283876	29.400180
360.071356	19140.896650	29.405197
360.429674	19166.791531	29.410215
360.779868	19208.350108	29.415232
361.096709	19242.277009	29.420250
361.697362	19265.997668	29.425268
361.568116	19319.652065	29.430285
362.217499	19350.243906	29.435303
362.441322	19389.594877	29.440320
362.936280	19427.562836	29.445338
363.270504	19482.462167	29.450356
363.279536	19524.924394	29.455373
363.982341	19551.451831	29.460391
364.265080	19592.631578	29.465408
364.867697	19633.850012	29.470426
365.602893	19658.455414	29.475444
365.441355	19700.944692	29.480461
366.241346	19730.618554	29.485479
366.427940	19769.494205	29.490496
366.710873	19797.281560	29.495514
367.000968	19829.562036	29.500532
366.940024	19872.892684	29.505549
367.643349	19898.019185	29.510567
368.187685	19935.828816	29.515584
368.442891	19979.903591	29.520602
369.175595	20013.102856	29.525620
368.903763	20039.714840	29.530637
369.891325	20067.127713	29.535655
370.021173	20098.338007	29.540672
370.166305	20128.604718	29.545690
370.769139	20166.811923	29.550708
371.130815	20210.349504	29.555725
371.621939	20237.866740	29.560743
372.294339	20275.518838	29.565760
372.592027	20302.223174	29.570778
372.831576	20324.163737	29.575796
372.930400	20376.015107	29.580813
373.160310	20394.661039	29.585831
373.514420	20431.131723	29.590848
373.832725	20468.953105	29.595866
374.264399	20503.293975	29.600884
374.651505	20552.103026	29.605901
375.142596	20589.916632	29.610919
375.390530	20619.774716	29.615936
375.652748	20660.596331	29.620954
376.399749	20695.519241	29.625972
376.552316	20747.293520	29.630989
376.968930	20778.413572	29.636007
377.273327	20817.820816	29.641024
377.603437	20858.704217	29.646042
377.972959	20888.460718	29.651060
378.156468	20948.016740	29.656077
378.857742	20987.831768	29.661095
379.044685	21029.399786	29.666112
379.764147	21057.646830	29.671130
380.759772	21094.520618	29.676148
380.753039	21142.814728	29.681165
380.993388	21161.325788	29.686183
381.709949	21200.213389	29.691200
381.811245	21241.936392	29.696218
382.359067	21268.626176	29.701236
382.747549	21301.318905	29.706253
383.215214	21340.301550	29.711271
383.927800	21377.076104	29.716288
384.264585	21399.236919	29.721306
384.877754	21423.945497	29.726324
384.933579	21461.525556	29.731341
385.250246	21493.554191	29.736359
385.656795	21513.108654	29.741376
386.000974	21541.174149	29.746394
386.235537	21571.340412	29.751412
386.459848	21607.770467	29.756429
386.648013	21641.108651	29.761447
387.193933	21674.222263	29.766464
387.663629	21712.704096	29.771482
388.016089	21745.012656	29.776500
387.990989	21798.282580	29.781517
388.713101	21823.692665	29.786535
389.009828	21871.241898	29.791552
389.452701	21920.165546	29.796570
390.260916	21947.310019	29.801588
390.457281	21977.661476	29.806605
391.064513	22013.478928	29.811623
391.367200	22039.696471	29.816640
391.865920	22074.820938	29.821658
392.335926	22112.376602	29.826676
392.735325	22140.392986	29.831693
393.048473	22160.835492	29.836711
393.321430	22192.305107	29.841728
393.622739	22234.681781	29.846746
394.281604	22253.504874	29.851764
394.073951	22290.066101	29.856781
394.734303	22332.211859	29.861799
394.899535	22351.723605	29.866816
395.378661	22390.019392	29.871834
395.768634	22412.508581	29.876852
396.013731	22459.185097	29.881869
396.210130	22492.214590	29.886887
396.881775	22526.854214	29.891904
396.908679	22573.578128	29.896922
397.320489	22603.426863	29.901940
397.698937	22653.616717	29.906957
398.190720	22695.125887	29.911975
398.732003	22732.128793	29.916992
398.929360	22775.060062	29.922010
399.414886	22818.544544	29.927028
399.865035	22850.894274	29.932045
400.009582	22895.680847	29.937063
400.801628	22940.212368	29.942080
400.863857	22986.643059	29.947098
401.074065	23037.121998	29.952116
401.425637	23077.535829	29.957133
402.017871	23131.666612	29.962151
402.372388	23174.495676	29.967168
402.917001	23229.492361	29.972186
403.657577	23274.504701	29.977204
403.862619	23317.951662	29.982221
404.197852	23362.671708	29.987239
404.790379	23397.671494	29.992256
405.005995	23450.995169	29.997274
405.813454	23492.514070	30.002292
406.322712	23522.770897	30.007309
406.600828	23564.203978	30.012327
407.232587	23602.436310	30.017344
407.397228	23644.604170	30.022362
408.161501	23671.646743	30.027380
408.487142	23725.959069	30.032397
408.559639	23763.073211	30.037415
409.044931	23794.808744	30.042432
409.433272	23841.722429	30.047450
410.122547	23878.350209	30.052468
410.672648	23925.552756	30.057485
410.783753	23962.519048	30.062503
411.008511	24003.284008	30.067520
411.212644	24031.499775	30.072538
411.764402	24084.352072	30.077556
412.030760	24145.053603	30.082573
412.604700	24183.802949	30.087591
413.129656	24224.198762	30.092608
413.489337	24276.028512	30.097626
413.790053	24318.246524	30.102644
414.191623	24365.757081	30.107661
414.389465	24396.957810	30.112679
414.927951	24439.721842	30.117696
415.170516	24505.950588	30.122714
415.890544	24535.185744	30.127732
416.390104	24575.391062	30.132749
416.506964	24641.532301	30.137767
417.292209	24681.307508	30.142784
417.323360	24706.101283	30.147802
418.447409	24749.855808	30.152820
418.561301	24811.065841	30.157837
419.121646	24849.667577	30.162855
419.867289	24876.888609	30.167872
420.236131	24925.571431	30.172890
420.837486	24954.483160	30.177908
421.299496	24976.629569	30.182925
421.706174	25015.471519	30.187943
422.283387	25049.635204	30.192960
422.016121	25076.875654	30.197978
422.799923	25111.046335	30.202996
422.908101	25149.105310	30.208013
423.401956	25172.889820	30.213031
423.734258	25214.283286	30.218048
423.891295	25246.738052	30.223066
424.734873	25281.635607	30.228084
424.704989	25326.009573	30.233101
424.925109	25376.233645	30.238119
425.478708	25400.311369	30.243136
425.608212	25451.465234	30.248154
426.446377	25497.937036	30.253172
426.858013	25543.515929	30.258189
426.951862	25579.629167	30.263207
427.524611	25632.416578	30.268224
427.467335	25689.996429	30.273242
428.130893	25738.850506	30.278260
428.412076	25781.933226	30.283277
428.913863	25841.687293	30.288295
429.771822	25890.169071	30.293312
429.788771	25941.442343	30.298330
430.620767	25985.144214	30.303348
430.980330	26026.984580	30.308365
431.103719	26083.094570	30.313383
431.895938	26124.084684	30.318400
432.263529	26172.951047	30.323418
432.829265	26227.761557	30.328436
433.122238	26286.887767	30.333453
433.745593	26332.580450	30.338471
434.463307	26373.924100	30.343488
434.563444	26425.459475	30.348506
435.086639	26466.557930	30.353524
435.727267	26506.876970	30.358541
435.965038	26542.213081	30.363559
436.616717	26583.858316	30.368576
436.887380	26630.275553	30.373594
437.077991	26680.629759	30.378612
438.139203	26717.640626	30.383629
438.316844	26769.583720	30.388647
439.260696	26806.475387	30.393664
439.537991	26858.679847	30.398682
439.708578	26895.891839	30.403700
440.297568	26950.524192	30.408717
440.468978	26985.052115	30.413735
440.794048	27028.506057	30.418752
441.769527	27084.812905	30.423770
441.614694	27117.688612	30.428788
442.250008	27158.584113	30.433805
441.944639	27205.457627	30.438823
442.935434	27259.993051	30.443840
443.222252	27306.892032	30.448858
443.886367	27359.800574	30.453876
444.763401	27413.721293	30.458893
445.143222	27456.735152	30.463911
445.605044	27493.824630	30.468928
445.891557	27543.752325	30.473946
446.322111	27589.688384	30.478964
447.376355	27615.924438	30.483981
447.364910	27674.250918	30.488999
448.013281	27707.550214	30.494016
448.531338	27756.342608	30.499034
448.742898	27773.542441	30.504052
449.421724	27821.305414	30.509069
449.761187	27871.442955	30.514087
450.084947	27897.885272	30.519104
450.356583	27950.538728	30.524122
450.741243	27987.522154	30.529140
451.471090	28020.032645	30.534157
451.657070	28064.644566	30.539175
452.047418	28102.926867	30.544192
452.765598	28143.050837	30.549210
453.053879	28185.523326	30.554228
453.436529	28224.762926	30.559245
453.368390	28279.769856	30.564263
453.991544	28314.856689	30.569280
454.608449	28368.211427	30.574298
454.905012	28399.100322	30.579316
455.606662	28455.974206	30.584333
455.872486	28503.539171	30.589351
456.393800	28550.793941	30.594368
456.587915	28611.231452	30.599386
456.915130	28663.641322	30.604404
457.447004	28711.213381	30.609421
457.604211	28763.134312	30.614439
458.012566	28811.894185	30.619456
458.516173	28877.514694	30.624474
458.856308	28944.253895	30.629492
459.302281	28997.424307	30.634509
459.714407	29063.183654	30.639527
460.299699	29127.693862	30.644544
460.838626	29187.142696	30.649562
461.518724	29235.937738	30.654580
462.330966	29302.310118	30.659597
462.421179	29369.716832	30.664615
463.052649	29403.293482	30.669632
463.661515	29461.526673	30.674650
464.287410	29512.353509	30.679668
465.099949	29556.868931	30.684685
465.516101	29612.875797	30.689703
466.390713	29649.062601	30.694720
466.600133	29706.160700	30.699738
466.950085	29761.412415	30.704756
467.691401	29793.451160	30.709773
467.978106	29843.312902	30.714791
468.304436	29879.351002	30.719808
468.854012	29937.740696	30.724826
468.884692	29981.979411	30.729844
469.301251	30038.344054	30.734861
469.854775	30090.436931	30.739879
469.998017	30149.146826	30.744896
471.023098	30200.297760	30.749914
471.286792	30255.129945	30.754932
471.991818	30291.011704	30.759949
472.201372	30364.551056	30.764967
472.575624	30411.311504	30.769984
473.085629	30464.273926	30.775002
473.617078	30520.409784	30.780020
473.784753	30568.012387	30.785037
474.556009	30636.453524	30.790055
474.911309	30696.265944	30.795072
475.414937	30748.028313	30.800090
475.675868	30815.696350	30.805108
476.626971	30880.799366	30.810125
476.834425	30921.550446	30.815143
477.345900	30982.382288	30.820160
478.215253	31035.593103	30.825178
478.593077	31095.034052	30.830196
479.100952	31148.216584	30.835213
479.181263	31202.501541	30.840231
479.617314	31254.964334	30.845248
480.200163	31312.258392	30.850266
480.867216	31376.470021	30.855284
481.649811	31414.190044	30.860301
481.965304	31475.809995	30.865319
482.862168	31514.243298	30.870336
483.492077	31549.509072	30.875354
483.770239	31598.288787	30.880372
483.992881	31622.440914	30.885389
484.568015	31677.055747	30.890407
484.647137	31719.233831	30.895424
485.176242	31766.029113	30.900442
485.659298	31814.788206	30.905460
486.080329	31849.574827	30.910477
486.548329	31925.308613	30.915495
486.855545	31981.252729	30.920512
487.528117	32021.951624	30.925530
487.765771	32063.508053	30.930548
488.367115	32121.454790	30.935565
489.135389	32190.845851	30.940583
489.748318	32234.445105	30.945600
490.285162	32289.692869	30.950618
490.284921	32339.691155	30.955636
490.863519	32384.615268	30.960653
491.362694	32443.684219	30.965671
491.761171	32505.950333	30.970688
492.323841	32561.901427	30.975706
492.449222	32623.402205	30.980724
493.255019	32693.868102	30.985741
493.717429	32744.040370	30.990759
494.086188	32805.441634	30.995776
495.063478	32872.942481	31.000794
495.436580	32922.170840	31.005812
495.652479	32972.078423	31.010829
495.777258	33041.374043	31.015847
496.240895	33103.773489	31.020864
497.156507	33173.901337	31.025882
496.998509	33241.890865	31.030900
497.946817	33313.667204	31.035917
498.359856	33383.326731	31.040935
498.663037	33441.904472	31.045952
499.360875	33511.735175	31.050970
500.019559	33581.395925	31.055988
500.580220	33638.518220	31.061005
501.330896	33700.919692	31.066023
501.850672	33771.853638	31.071040
502.507925	33829.623212	31.076058
502.846918	33892.014475	31.081076
503.456002	33947.760353	31.086093
503.618527	34012.339447	31.091111
504.229432	34063.730991	31.096128
504.778049	34134.488079	31.101146
505.241929	34201.359379	31.106164
505.993491	34252.056137	31.111181
506.713754	34316.111921	31.116199
506.847022	34382.319077	31.121216
507.522311	34443.025374	31.126234
507.750091	34506.629923	31.131252
508.216355	34563.666662	31.136269
508.573042	34640.695814	31.141287
509.535229	34706.587398	31.146304
510.197420	34773.560625	31.151322
510.008134	34850.554647	31.156340
510.504718	34902.450295	31.161357
510.732365	34958.587370	31.166375
511.315355	35037.442620	31.171392
512.325620	35098.335647	31.176410
512.342072	35187.988783	31.181428
512.899648	35249.376790	31.186445
513.588915	35326.215126	31.191463
514.384945	35399.653349	31.196480
514.925418	35453.373605	31.201498
515.570550	35515.678974	31.206516
516.182581	35561.438713	31.211533
516.663979	35626.296022	31.216551
516.936604	35681.803125	31.221568
517.970089	35730.923885	31.226586
518.097311	35791.753710	31.231604
518.570798	35850.532153	31.236621
518.959914	35912.057558	31.241639
519.722964	35976.642407	31.246656
520.283740	36022.982979	31.251674
520.564706	36093.536447	31.256692
521.012600	36156.870686	31.261709
521.577322	36213.877506	31.266727
521.946117	36270.692811	31.271744
522.662796	36332.774620	31.276762
523.232997	36401.643682	31.281780
523.669678	36471.264051	31.286797
524.053115	36531.656437	31.291815
524.554594	36613.637420	31.296832
525.050284	36666.639724	31.301850
525.476639	36734.476621	31.306868
526.043357	36802.401044	31.311885
526.664346	36863.285492	31.316903
526.821432	36944.788375	31.321920
527.689544	37006.219484	31.326938
528.222018	37078.849729	31.331956
528.796172	37151.681674	31.336973
529.560098	37226.051064	31.341991
530.028122	37300.520132	31.347008
530.819679	37353.510310	31.352026
530.881590	37435.409848	31.357044
531.430329	37509.490889	31.362061
531.941701	37565.642920	31.367079
532.683843	37636.249355	31.372096
533.661606	37718.282946	31.377114
533.947802	37770.073323	31.382132
534.616816	37825.272255	31.387149
535.272990	37903.768242	31.392167
535.525643	37970.391849	31.397184
536.307635	38016.161341	31.402202
536.874295	38100.552722	31.407220
537.529183	38170.295114	31.412237
537.821005	38216.133451	31.417255
537.986115	38285.660512	31.422272
538.696784	38363.682392	31.427290
539.340381	38420.307599	31.432308
540.202676	38470.019619	31.437325
540.871115	38555.248471	31.442343
540.793051	38631.504930	31.447360
541.372935	38686.768560	31.452378
541.798687	38755.430610	31.457396
542.591910	38831.266253	31.462413
543.380384	38901.503862	31.467431
543.694189	38970.848025	31.472448
543.978874	39031.356623	31.477466
544.659030	39110.216852	31.482484
545.116854	39181.816851	31.487501
546.068096	39248.957872	31.492519
546.265630	39321.210575	31.497536
547.182440	39381.975751	31.502554
547.856011	39447.957664	31.507572
548.499080	39517.120119	31.512589
549.192482	39583.140279	31.517607
549.453413	39642.540649	31.522624
549.951756	39691.167224	31.527642
550.287266	39765.564163	31.532660
550.840315	39820.744145	31.537677
551.402372	39888.355828	31.542695
551.737419	39960.739863	31.547712
552.415983	40016.786657	31.552730
552.972735	40075.647178	31.557748
553.137532	40158.637298	31.562765
553.889759	40217.639596	31.567783
554.420961	40283.701713	31.572800
554.840908	40351.777335	31.577818
555.397412	40432.466064	31.582836
555.729691	40498.498685	31.587853
556.333799	40557.785380	31.592871
556.671919	40648.091134	31.597888
557.499098	40716.915238	31.602906
557.935033	40786.220886	31.607924
558.578925	40865.082077	31.612941
559.384398	40940.248982	31.617959
559.596945	41013.465503	31.622976
560.022081	41080.902196	31.627994
560.736155	41165.924241	31.633012
560.949323	41243.642908	31.638029
561.868157	41327.555474	31.643047
562.786769	41414.211593	31.648064
563.308508	41477.059795	31.653082
563.591564	41560.737518	31.658100
564.337281	41646.962418	31.663117
564.953075	41706.995885	31.668135
565.416013	41782.623722	31.673152
566.014344	41860.322420	31.678170
566.890863	41935.910988	31.683188
567.195738	42013.103214	31.688205
568.100851	42082.339424	31.693223
568.031507	42171.940253	31.698240
568.969846	42242.525839	31.703258
569.421900	42326.823119	31.708276
569.888566	42399.703293	31.713293
570.873203	42470.724063	31.718311
571.394620	42563.543899	31.723328
572.185015	42621.976245	31.728346
572.415726	42695.546873	31.733364
572.833332	42782.289032	31.738381
574.148542	42856.198909	31.743399
574.353161	42938.424727	31.748416
575.084621	43002.967177	31.753434
575.778245	43087.398506	31.758452
575.739767	43155.194026	31.763469
576.320618	43231.597568	31.768487
577.092082	43324.032659	31.773504
577.766846	43393.848527	31.778522
578.788203	43464.996495	31.783540
579.387944	43537.600304	31.788557
580.309833	43596.569651	31.793575
580.744940	43666.912314	31.798592
580.878436	43731.938071	31.803610
582.204058	43801.695334	31.808628
582.319820	43873.909993	31.813645
583.217022	43930.785028	31.818663
583.700790	43999.902281	31.823680
584.165378	44075.040409	31.828698
584.577983	44147.169218	31.833716
584.810683	44222.718782	31.838733
585.607067	44315.549342	31.843751
585.910431	44379.090703	31.848768
586.382472	44450.948829	31.853786
586.985036	44540.124944	31.858804
587.432012	44607.558279	31.863821
588.448687	44684.615664	31.868839
588.990590	44765.856176	31.873856
589.287241	44838.139416	31.878874
590.078455	44921.236929	31.883892
590.291000	44996.931880	31.888909
591.203392	45076.470777	31.893927
591.528045	45142.502317	31.898944
592.034228	45224.110655	31.903962
592.430866	45302.542237	31.908980
592.783963	45374.770872	31.913997
593.764741	45463.702652	31.919015
594.172669	45550.961348	31.924032
594.727027	45621.525340	31.929050
595.232525	45708.029829	31.934068
595.443048	45795.123350	31.939085
596.329709	45881.527797	31.944103
597.026297	45981.304178	31.949120
597.011516	46061.527689	31.954138
598.214952	46148.904063	31.959156
598.710287	46242.984287	31.964173
599.520128	46336.343650	31.969191
600.191385	46431.150402	31.974208
600.636546	46508.117088	31.979226
601.117292	46587.983143	31.984244
602.125540	46682.909171	31.989261
602.968591	46763.429739	31.994279
603.462268	46847.882701	31.999296
604.074130	46936.841350	32.004314
604.913560	47006.220418	32.009332
605.503067	47112.414638	32.014349
606.060690	47193.779908	32.019367
606.813446	47272.381936	32.024384
607.143905	47346.636471	32.029402
607.933330	47436.427035	32.034420
608.458473	47524.446004	32.039437
609.268733	47605.888161	32.044455
609.757386	47697.984244	32.049472
610.101935	47771.227651	32.054490
611.089212	47856.563554	32.059508
611.372789	47939.445650	32.064525
612.176857	48017.328650	32.069543
613.186476	48105.327147	32.074560
613.638459	48196.345434	32.079578
614.238329	48276.328428	32.084596
615.145367	48361.477761	32.089613
615.829640	48429.788760	32.094631
616.504434	48515.507660	32.099648
616.804513	48594.051000	32.104666
617.631099	48673.072968	32.109684
617.836201	48749.870540	32.114701
618.653998	48833.732522	32.119719
619.407324	48930.294056	32.124736
619.672879	48999.532057	32.129754
620.526401	49087.384047	32.134772
620.828174	49182.101404	32.139789
621.681651	49267.791028	32.144807
622.385606	49346.662361	32.149824
622.883369	49436.068447	32.154842
623.474577	49521.710947	32.159860
623.928526	49596.193898	32.164877
624.743113	49688.012106	32.169895
625.214290	49776.416761	32.174912
625.622071	49863.556430	32.179930
626.490313	49946.123325	32.184948
626.891083	50039.249539	32.189965
628.059869	50123.296088	32.194983
628.386398	50221.668459	32.200000
628.985472	50300.068383	32.205018
630.171137	50380.816168	32.210036
630.354647	50488.277460	32.215053
631.009770	50559.721193	32.220071
631.929613	50634.905003	32.225088
632.287972	50724.122218	32.230106
633.095445	50792.051823	32.235124
633.458111	50881.951239	32.240141
634.347623	50947.246501	32.245159
634.910017	51037.236829	32.250176
634.863803	51113.715884	32.255194
635.717214	51183.297387	32.260212
636.048749	51283.076654	32.265229
636.915389	51367.042753	32.270247
637.547175	51459.641850	32.275264
637.666504	51558.393230	32.280282
638.549924	51638.239244	32.285300
638.638515	51724.814722	32.290317
639.280297	51833.496463	32.295335
640.130227	51944.889107	32.300352
640.964188	52033.421109	32.305370
641.925683	52125.788921	32.310388
642.468718	52223.545142	32.315405
642.935357	52312.189622	32.320423
644.305959	52400.887360	32.325440
644.879767	52503.418716	32.330458
645.858259	52581.916884	32.335476
646.311847	52663.458451	32.340493
647.127602	52760.095281	32.345511
648.275250	52831.737736	32.350528
648.570022	52932.674995	32.355546
649.345752	53001.284090	32.360564
649.853108	53089.584277	32.365581
650.612373	53175.625909	32.370599
651.129345	53261.050942	32.375616
651.628896	53347.578438	32.380634
652.172501	53444.206767	32.385652
652.674677	53535.087303	32.390669
653.179596	53619.094495	32.395687
654.154662	53721.275417	32.400704
654.606086	53807.895035	32.405722
655.488038	53898.278642	32.410740
655.837935	53997.847749	32.415757
656.296060	54088.731826	32.420775
657.188695	54194.965754	32.425792
657.664570	54299.626511	32.430810
658.180693	54387.337280	32.435828
658.677003	54481.855838	32.440845
659.198923	54589.606199	32.445863
660.038512	54699.389543	32.450880
660.505036	54814.712623	32.455898
661.561031	54915.224858	32.460916
662.241491	55015.249977	32.465933
662.635392	55121.981967	32.470951
663.487513	55215.049053	32.475968
663.810766	55328.282318	32.480986
664.718378	55438.469234	32.486004
665.411174	55536.637491	32.491021
666.107740	55646.550847	32.496039
666.968960	55747.156376	32.501056
667.176767	55852.476229	32.506074
668.188141	55955.983311	32.511092
668.563038	56060.954459	32.516109
669.304786	56170.319916	32.521127
670.335331	56278.425182	32.526144
670.823319	56384.175472	32.531162
671.950259	56481.379546	32.536180
672.441149	56577.937260	32.541197
673.016241	56680.136481	32.546215
674.064037	56782.157069	32.551232
674.678055	56887.510136	32.556250
675.476955	56991.348390	32.561268
675.787446	57085.215113	32.566285
676.616398	57169.468317	32.571303
676.976685	57266.828140	32.576320
677.659572	57369.531241	32.581338
678.478681	57448.858759	32.586356
679.245388	57547.542937	32.591373
680.059573	57645.392018	32.596391
680.882288	57733.206065	32.601408
681.365534	57825.701876	32.606426
681.929805	57911.524761	32.611444
683.108690	58001.884506	32.616461
683.399394	58090.849550	32.621479
684.132095	58192.259639	32.626496
684.774287	58287.656978	32.631514
685.423872	58378.421790	32.636532
686.795732	58476.195500	32.641549
687.156396	58552.690104	32.646567
688.300707	58629.200921	32.651584
688.536823	58738.923129	32.656602
689.278695	58821.510539	32.661620
690.166529	58912.099415	32.666637
690.641577	59004.412479	32.671655
691.177667	59094.554743	32.676672
691.344221	59192.625803	32.681690
691.995308	59299.413651	32.686708
692.863585	59402.684303	32.691725
693.554501	59500.379588	32.696743
694.400949	59600.065520	32.701760
695.416486	59704.267621	32.706778
696.146604	59789.824734	32.711796
697.117800	59891.886552	32.716813
697.672726	59996.924567	32.721831
698.625021	60097.372779	32.726848
698.815295	60191.387713	32.731866
699.610721	60268.657561	32.736884
700.350510	60366.816635	32.741901
700.910511	60484.040427	32.746919
701.271048	60579.678464	32.751936
702.125670	60676.815267	32.756954
702.606655	60790.622329	32.761972
703.478672	60903.373262	32.766989
704.005526	61020.232780	32.772007
704.672533	61109.553533	32.777024
705.334043	61232.509579	32.782042
706.313446	61340.644399	32.787060
706.754923	61452.515200	32.792077
707.104524	61569.230205	32.797095
708.113299	61672.919051	32.802112
708.866633	61791.938644	32.807130
709.549981	61902.015027	32.812148
710.532823	62014.911852	32.817165
711.348375	62129.846719	32.822183
712.070635	62225.666639	32.827200
712.734905	62345.133951	32.832218
713.478308	62447.366382	32.837236
714.399600	62542.731475	32.842253
714.996105	62652.940031	32.847271
715.799206	62762.754809	32.852288
716.511831	62879.771323	32.857306
717.087213	62991.887615	32.862324
717.764687	63091.384812	32.867341
718.827801	63196.772640	32.872359
719.369278	63301.014669	32.877376
720.013319	63409.380209	32.882394
720.703797	63516.101640	32.887412
721.812945	63613.596013	32.892429
721.774565	63724.654701	32.897447
722.737502	63841.085491	32.902464
723.264083	63960.231035	32.907482
724.235718	64058.211642	32.912500
724.900871	64160.731038	32.917517
725.338478	64271.669834	32.922535
726.104116	64382.112603	32.927552
726.464644	64493.722688	32.932570
727.250838	64600.579332	32.937588
728.133216	64705.701368	32.942605
728.669393	64820.590040	32.947623
729.532906	64922.113373	32.952640
730.121174	65044.737855	32.957658
730.770703	65148.705937	32.962676
731.915407	65265.639422	32.967693
732.488292	65375.708481	32.972711
733.366493	65490.089280	32.977728
733.863151	65607.542591	32.982746
734.294927	65724.956713	32.987764
735.134803	65835.274901	32.992781
735.702013	65964.532963	32.997799
736.298927	66082.585574	33.002816
737.334532	66206.628577	33.007834
737.982883	66330.211597	33.012852
739.109378	66447.426585	33.017869
739.736950	66588.088718	33.022887
740.266083	66699.461606	33.027904
741.065357	66829.382091	33.032922
741.637532	66954.997972	33.037940
742.490792	67076.016636	33.042957
743.180027	67206.248436	33.047975
743.641451	67338.857692	33.052992
744.293486	67488.138315	33.058010
745.173299	67620.528545	33.063028
745.798958	67757.563862	33.068045
746.396939	67895.692005	33.073063
747.264610	68025.033344	33.078080
748.363992	68169.181117	33.083098
748.906700	68295.277737	33.088116
749.923038	68426.221749	33.093133
750.414225	68562.949468	33.098151
751.319396	68690.455321	33.103168
752.335511	68839.223928	33.108186
752.924803	68969.413644	33.113204
753.979800	69100.456626	33.118221
754.569505	69226.987303	33.123239
755.765732	69361.612271	33.128256
756.496512	69482.823105	33.133274
757.118527	69611.519311	33.138292
758.126120	69742.182121	33.143309
758.970268	69873.789483	33.148327
759.819192	69991.759279	33.153344
760.555033	70121.672675	33.158362
761.145816	70240.685444	33.163380
761.928359	70365.212126	33.168397
762.751018	70493.526493	33.173415
763.494454	70612.275877	33.178432
764.578436	70727.713499	33.183450
765.098233	70866.512589	33.188468
766.253439	70990.684231	33.193485
766.873053	71105.941354	33.198503
767.550912	71235.965981	33.203520
768.529664	71356.925274	33.208538
769.111451	71473.436239	33.213556
770.156787	71589.333842	33.218573
770.711002	71717.029678	33.223591
771.610869	71838.023694	33.228608
772.595411	71948.969710	33.233626
772.736037	72074.807444	33.238644
773.584246	72196.785776	33.243661
774.332276	72319.875254	33.248679
775.034929	72443.630544	33.253696
775.549049	72567.379742	33.258714
776.492435	72684.324475	33.263732
777.313794	72804.641351	33.268749
777.801278	72931.748402	33.273767
778.688097	73050.949260	33.278784
779.537756	73164.775684	33.283802
780.049522	73293.879063	33.288820
780.824983	73401.092005	33.293837
781.444920	73547.359965	33.298855
782.082037	73683.464096	33.303872
783.170132	73796.400798	33.308890
783.529661	73927.544010	33.313908
784.538824	74072.606671	33.318925
785.503779	74198.617898	33.323943
786.227254	74326.800841	33.328960
786.824722	74455.074911	33.333978
787.610928	74599.419060	33.338996
788.495769	74725.231566	33.344013
789.510210	74863.310764	33.349031
789.894095	75005.807901	33.354048
791.198025	75140.476712	33.359066
791.869016	75269.869120	33.364084
792.416017	75407.826591	33.369101
792.849915	75544.102425	33.374119
793.939122	75697.295523	33.379136
794.975005	75838.356037	33.384154
795.200388	75973.467383	33.389172
796.529474	76115.278121	33.394189
797.464370	76269.487296	33.399207
798.296277	76412.779736	33.404224
798.907002	76556.780022	33.409242
799.736049	76694.003343	33.414260
800.511295	76837.276288	33.419277
801.041071	76984.720616	33.424295
802.067084	77134.563221	33.429312
802.721748	77278.036035	33.434330
803.634674	77437.873293	33.439348
804.125050	77590.229789	33.444365
804.706789	77731.396427	33.449383
806.055477	77883.379198	33.454400
806.934538	78039.754097	33.459418
807.357181	78198.444473	33.464436
808.422407	78337.498532	33.469453
809.040502	78492.515588	33.474471
809.564869	78644.842102	33.479488
810.505116	78797.967519	33.484506
811.425965	78956.131965	33.489524
812.260358	79100.750726	33.494541
813.242922	79267.990090	33.499559
813.853433	79416.904718	33.504576
814.914145	79579.857667	33.509594
816.023393	79735.630888	33.514612
816.699927	79874.113552	33.519629
817.707548	80009.683326	33.524647
818.311600	80176.106438	33.529664
819.557999	80327.325796	33.534682
819.925925	80474.750432	33.539700
820.740239	80622.943627	33.544717
821.754513	80783.895155	33.549735
822.895277	80914.912958	33.554752
823.935846	81054.316948	33.559770
824.525877	81199.394461	33.564788
825.381573	81341.342067	33.569805
826.316345	81474.389757	33.574823
826.803550	81643.379669	33.579840
828.021156	81764.129200	33.584858
828.837394	81918.131431	33.589876
829.450157	82063.096873	33.594893
830.505201	82201.474427	33.599911
830.701139	82330.980075	33.604928
831.738299	82471.626953	33.609946
832.574347	82618.887077	33.614964
833.207415	82756.192665	33.619981
833.955704	82899.236896	33.624999
834.548898	83046.160316	33.630016
835.634954	83188.574906	33.635034
836.379750	83341.099258	33.640052
836.869342	83491.623354	33.645069
837.790480	83652.174128	33.650087
838.157370	83811.988783	33.655104
839.219223	83968.355738	33.660122
839.937779	84126.286163	33.665140
840.786361	84287.568275	33.670157
841.849237	84447.784896	33.675175
842.038436	84609.329986	33.680192
843.094373	84767.734230	33.685210
844.065695	84945.918340	33.690228
844.796466	85115.994615	33.695245
845.790607	85280.941865	33.700263
846.425002	85452.795403	33.705280
847.440747	85619.569981	33.710298
847.981457	85804.348582	33.715316
848.861548	85972.704547	33.720333
849.737603	86151.350255	33.725351
850.643355	86335.743809	33.730368
851.703880	86499.473973	33.735386
852.584282	86675.168199	33.740404
853.227159	86853.775558	33.745421
854.290580	87040.799803	33.750439
855.073902	87212.047011	33.755456
855.966771	87377.139784	33.760474
857.086253	87554.996783	33.765492
857.664616	87740.335033	33.770509
858.818879	87918.733223	33.775527
859.231318	88098.919425	33.780544
860.456930	88276.796022	33.785562
860.940935	88458.365253	33.790580
861.889766	88641.801760	33.795597
862.968575	88819.637102	33.800615
863.830742	89008.159354	33.805632
864.995183	89178.187333	33.810650
865.787851	89373.039233	33.815668
866.812881	89548.079332	33.820685
867.656122	89727.080466	33.825703
868.164356	89908.612559	33.830720
868.987396	90083.367233	33.835738
870.142955	90266.674642	33.840756
870.901119	90450.207290	33.845773
871.750408	90621.848092	33.850791
872.260702	90806.936880	33.855808
873.584553	90996.455547	33.860826
874.011888	91188.775368	33.865844
874.903234	91369.426316	33.870861
875.907981	91553.736787	33.875879
876.571269	91747.123304	33.880896
878.027630	91926.792833	33.885914
879.069445	92117.980759	33.890932
879.900160	92283.769860	33.895949
880.962980	92476.020395	33.900967
881.611478	92658.265369	33.905984
882.594962	92835.905944	33.911002
883.382070	93017.295332	33.916020
884.190150	93201.467369	33.921037
885.354653	93384.398431	33.926055
886.246206	93571.901231	33.931072
887.154027	93741.738222	33.936090
887.779260	93912.142052	33.941108
888.577204	94072.189299	33.946125
889.460343	94249.223891	33.951143
890.590587	94427.048109	33.956160
891.564908	94586.120220	33.961178
892.297645	94759.056623	33.966196
893.225136	94927.531498	33.971213
894.328458	95097.288702	33.976231
894.774800	95291.707755	33.981248
895.991406	95448.017451	33.986266
896.933411	95616.342762	33.991284
897.537912	95809.328303	33.996301
898.420655	95979.995205	34.001319
899.621548	96156.630345	34.006336
900.478496	96332.646255	34.011354
901.196090	96517.377293	34.016372
901.868063	96707.978717	34.021389
903.295323	96867.585844	34.026407
904.222939	97064.040965	34.031424
905.078781	97227.504768	34.036442
906.274379	97405.833503	34.041460
907.016593	97577.920933	34.046477
908.255024	97761.771337	34.051495
908.851235	97937.411258	34.056512
910.419585	98100.066840	34.061530
911.532943	98269.090910	34.066548
912.301879	98439.698600	34.071565
913.549671	98607.829183	34.076583
913.929702	98777.585489	34.081600
915.193888	98951.286437	34.086618
916.221132	99108.600074	34.091636
916.946424	99282.354310	34.096653
918.219273	99452.189341	34.101671
918.711024	99621.717674	34.106688
919.480164	99797.209151	34.111706
920.432490	99972.424708	34.116724
920.967512	100144.158829	34.121741
922.354293	100312.214571	34.126759
923.241082	100499.276867	34.131776
924.231614	100666.678674	34.136794
925.008980	100844.347563	34.141812
925.980738	101024.176119	34.146829
926.961753	101208.752685	34.151847
927.731329	101378.443183	34.156864
928.667113	101564.454288	34.161882
929.598427	101734.873861	34.166900
930.839920	101908.845809	34.171917
931.954866	102076.584576	34.176935
932.731436	102254.883904	34.181952
933.778203	102421.300291	34.186970
934.781529	102610.644472	34.191988
935.380278	102780.695392	34.197005
936.505653	102943.993472	34.202023
937.141587	103134.617815	34.207040
938.267799	103329.227473	34.212058
939.085399	103496.657392	34.217076
940.040154	103681.224467	34.222093
941.155023	103857.769521	34.227111
941.733812	104033.486190	34.232128
942.599344	104214.051161	34.237146
944.017033	104388.675640	34.242164
944.455166	104582.895468	34.247181
945.581075	104765.941369	34.252199
946.512805	104941.675569	34.257216
947.464323	105131.464690	34.262234
948.556953	105307.307764	34.267252
949.444748	105496.388212	34.272269
950.274406	105667.623057	34.277287
951.439499	105844.781199	34.282304
952.567057	106017.792813	34.287322
953.250878	106182.735573	34.292340
954.156768	106360.243942	34.297357
954.998342	106529.747407	34.302375
955.821809	106701.749906	34.307392
956.539796	106886.891690	34.312410
957.429681	107063.900855	34.317428
958.043193	107247.669280	34.322445
959.038303	107434.567579	34.327463
959.706485	107616.277796	34.332480
960.582413	107816.471565	34.337498
961.660599	108000.155828	34.342516
961.999320	108210.674867	34.347533
963.247460	108403.389654	34.352551
964.360993	108619.128859	34.357568
965.194531	108825.606715	34.362586
966.168349	109028.643231	34.367604
967.176397	109240.301139	34.372621
968.197897	109444.662862	34.377639
969.327328	109656.266017	34.382656
969.991682	109870.886190	34.387674
971.014161	110072.111300	34.392692
971.875808	110298.064005	34.397709
972.883708	110508.085285	34.402727
974.095141	110723.597247	34.407744
974.772608	110933.866389	34.412762
976.316037	111149.301596	34.417780
977.017622	111369.488266	34.422797
978.409753	111565.140673	34.427815
979.123680	111790.788207	34.432832
980.154322	112003.971430	34.437850
981.411652	112205.224274	34.442868
982.536814	112426.426276	34.447885
983.645361	112624.767929	34.452903
984.800995	112843.143411	34.457920
985.489688	113041.620735	34.462938
986.724714	113258.288938	34.467956
987.392952	113479.511527	34.472973
988.349917	113673.908056	34.477991
989.272056	113884.742221	34.483008
990.205838	114115.807186	34.488026
991.480431	114319.999015	34.493044
992.181253	114540.502621	34.498061
993.384759	114769.159510	34.503079
994.510469	114973.393394	34.508096
995.369181	115198.728223	34.513114
996.993763	115407.380315	34.518132
997.497421	115621.818674	34.523149
998.872065	115832.554896	34.528167
999.826382	116036.698163	34.533184
1000.783103	116261.759323	34.538202
1001.822120	116454.476718	34.543220
1002.858275	116673.763547	34.548237
1004.290561	116879.633074	34.553255
1004.931912	117085.013875	34.558272
1006.176851	117297.670250	34.563290
1007.353263	117505.867120	34.568308
1008.441449	117717.222203	34.573325
1009.028775	117926.026204	34.578343
1010.474569	118124.680700	34.583360
1010.926913	118328.619316	34.588378
1012.109765	118534.820783	34.593396
1012.866963	118768.917972	34.598413
1013.502658	118971.297798	34.603431
1014.548209	119197.824680	34.608448
1015.443603	119418.562341	34.613466
1016.753723	119621.418258	34.618484
1017.503635	119835.226937	34.623501
1018.712246	120040.433985	34.628519
1019.840666	120240.549341	34.633536
1020.291791	120452.726684	34.638554
1021.526852	120652.155717	34.643572
1022.313902	120884.592584	34.648589
1023.380462	121086.371255	34.653607
1024.215150	121298.238029	34.658624
1024.991135	121523.877286	34.663642
1026.376202	121734.389217	34.668660
1027.252302	121980.948962	34.673677
1027.975361	122203.358246	34.678695
1029.124555	122408.300360	34.683712
1030.006027	122650.759158	34.688730
1031.105959	122881.500218	34.693748
1032.115522	123113.892717	34.698765
1033.107122	123347.836030	34.703783
1034.147393	123578.820492	34.708800
1035.262310	123816.916371	34.713818
1036.298279	124052.999580	34.718836
1037.215650	124287.520157	34.723853
1038.481786	124534.695816	34.728871
1039.718119	124776.492461	34.733888
1040.356410	125013.738802	34.738906
1041.665623	125263.257882	34.743924
1042.550694	125498.705759	34.748941
1043.513663	125741.239672	34.753959
1044.792808	125986.207330	34.758976
1045.674241	126231.293331	34.763994
1047.054491	126473.967025	34.769012
1048.004132	126721.656504	34.774029
1049.002680	126963.547997	34.779047
1050.675731	127209.220957	34.784064
1051.150594	127452.939123	34.789082
1052.365687	127692.101091	34.794100
1053.724541	127939.124565	34.799117
1054.671535	128185.761751	34.804135
1055.913441	128416.445832	34.809152
1056.909809	128662.850561	34.814170
1058.142833	128896.670320	34.819188
1059.242377	129143.911064	34.824205
1060.344606	129378.427827	34.829223
1061.768987	129614.325450	34.834240
1062.375186	129862.325149	34.839258
1063.642391	130104.780082	34.844276
1064.848901	130342.506396	34.849293
1065.876951	130578.971103	34.854311
1067.131888	130820.799866	34.859328
1068.098668	131054.375617	34.864346
1069.219975	131290.513419	34.869364
1070.404893	131533.259206	34.874381
1071.413327	131765.717910	34.879399
1072.712521	132002.528860	34.884416
1073.441042	132235.265399	34.889434
1074.737479	132470.102855	34.894452
1075.459014	132717.535656	34.899469
1076.571980	132952.597114	34.904487
1077.405968	133199.178466	34.909504
1078.623952	133445.064510	34.914522
1079.780420	133689.542830	34.919540
1080.709343	133923.868556	34.924557
1081.666673	134167.736890	34.929575
1082.982300	134419.204738	34.934592
1083.469612	134672.915661	34.939610
1084.655554	134926.094906	34.944628
1085.793562	135178.954441	34.949645
1086.779659	135419.987815	34.954663
1088.179522	135654.108919	34.959680
1089.197820	135901.605986	34.964698
1090.484030	136130.488152	34.969716
1091.783305	136365.759277	34.974733
1092.472458	136610.146653	34.979751
1093.474044	136832.120664	34.984768
1094.387866	137079.276237	34.989786
1095.684231	137321.743058	34.994804
1096.810160	137554.591796	34.999821
1097.748269	137806.084707	35.004839
1098.509474	138042.737147	35.009856
1099.171101	138296.054373	35.014874
1100.333251	138548.162523	35.019892
1101.674679	138809.536354	35.024909
1102.285318	139069.169112	35.029927
1103.372162	139330.094577	35.034944
1104.274392	139610.654030	35.039962
1105.199524	139871.293428	35.044980
1106.423229	140144.932288	35.049997
1107.362253	140426.532148	35.055015
1108.822150	140700.783158	35.060032
1109.994495	140982.285730	35.065050
1110.790601	141267.162081	35.070068
1112.089358	141539.557224	35.075085
1113.063691	141823.838225	35.080103
1114.696883	142115.316375	35.085120
1115.585479	142382.130755	35.090138
1116.906890	142667.718203	35.095156
1118.244331	142949.831029	35.100173
1118.999386	143223.686055	35.105191
1120.521196	143509.247380	35.110208
1121.340197	143788.358629	35.115226
1122.356269	144062.494194	35.120244
1123.311695	144353.862168	35.125261
1124.512542	144653.713487	35.130279
1126.131182	144929.227341	35.135296
1127.258195	145218.786186	35.140314
1128.360956	145516.441900	35.145332
1129.699774	145791.501450	35.150349
1130.838233	146077.413286	35.155367
1132.156980	146350.400767	35.160384
1133.209467	146643.356795	35.165402
1134.432615	146907.385885	35.170420
1136.060948	147178.984366	35.175437
1137.680060	147463.940263	35.180455
1139.178153	147733.154916	35.185472
1140.247142	147999.183168	35.190490
1141.464540	148251.543066	35.195508
1142.699098	148513.730498	35.200525
1143.330953	148797.579004	35.205543
1144.732926	149046.464414	35.210560
1145.655305	149319.095958	35.215578
1146.834740	149594.921129	35.220596
1148.123022	149858.491755	35.225613
1148.767470	150135.106839	35.230631
1150.100912	150410.101024	35.235648
1151.179279	150678.835999	35.240666
1152.115742	150952.200250	35.245684
1153.567356	151229.679557	35.250701
1154.373499	151509.804104	35.255719
1155.773674	151766.964892	35.260736
1157.047872	152057.784325	35.265754
1157.920662	152341.277859	35.270772
1159.154606	152603.900324	35.275789
1159.837380	152894.811180	35.280807
1161.358871	153161.943472	35.285824
1162.534183	153446.473489	35.290842
1163.668036	153721.880109	35.295860
1164.780710	153998.712820	35.300877
1165.886039	154264.120437	35.305895
1167.148518	154529.072696	35.310912
1168.186223	154793.290152	35.315930
1169.085557	155064.229574	35.320948
1170.790234	155329.025566	35.325965
1171.569414	155599.975898	35.330983
1172.598263	155861.119802	35.336000
1173.725622	156147.859504	35.341018
1174.452787	156430.506779	35.346036
1175.717101	156703.642604	35.351053
1176.581309	156995.112668	35.356071
1177.908722	157278.770574	35.361088
1179.150593	157557.205696	35.366106
1179.888137	157857.988553	35.371124
1181.586930	158149.811430	35.376141
1182.611540	158458.137263	35.381159
1183.769534	158752.806564	35.386176
1184.911559	159060.521455	35.391194
1186.032346	159356.254246	35.396212
1187.254828	159650.285220	35.401229
1188.086424	159970.566492	35.406247
1189.745366	160271.595980	35.411264
1190.802411	160564.772896	35.416282
1191.944220	160875.559000	35.421300
1193.513269	161179.362943	35.426317
1194.742765	161489.619108	35.431335
1195.973845	161796.769178	35.436352
1197.438805	162091.437447	35.441370
1198.434958	162405.798721	35.446388
1199.358101	162696.247279	35.451405
1200.443840	163012.818539	35.456423
1202.214676	163326.158140	35.461440
1203.436134	163623.973075	35.466458
1204.596471	163926.773551	35.471476
1205.964706	164240.731983	35.476493
1207.209114	164557.808885	35.481511
1208.595675	164863.078128	35.486528
1209.442958	165166.395897	35.491546
1210.511025	165481.110864	35.496564
1212.111843	165782.329371	35.501581
1213.226206	166114.816741	35.506599
1214.484541	166412.822759	35.511616
1215.188224	166732.859794	35.516634
1216.488335	167050.263142	35.521652
1218.022513	167368.848230	35.526669
1218.996059	167692.882601	35.531687
1220.306478	168016.977959	35.536704
1221.637749	168338.661472	35.541722
1222.585528	168653.495409	35.546740
1223.728691	168967.550709	35.551757
1225.061292	169314.427907	35.556775
1226.188837	169631.129711	35.561792
1227.461600	169951.248465	35.566810
1228.742737	170277.940989	35.571828
1230.225284	170597.674427	35.576845
1231.216038	170918.557187	35.581863
1232.568639	171245.930121	35.586880
1233.912946	171579.664118	35.591898
1234.925077	171899.776212	35.596916
1236.678054	172220.961070	35.601933
1237.656746	172545.892496	35.606951
1238.915457	172865.615296	35.611968
1240.574264	173175.972681	35.616986
1241.502367	173512.035437	35.622004
1242.772845	173829.009217	35.627021
1244.089016	174150.330269	35.632039
1245.006610	174482.188627	35.637056
1246.536398	174793.009471	35.642074
1247.663768	175102.947004	35.647092
1249.106459	175411.146694	35.652109
1250.296377	175717.346935	35.657127
1251.636149	176032.230085	35.662144
1252.725528	176334.186842	35.667162
1254.039032	176635.308982	35.672180
1255.513988	176941.089229	35.677197
1256.390015	177261.564703	35.682215
1257.438967	177572.000610	35.687232
1258.426515	177888.578364	35.692250
1259.715693	178206.555151	35.697268
1261.080971	178532.999116	35.702285
1262.154015	178861.232163	35.707303
1263.100873	179178.243689	35.712320
1264.636386	179516.900439	35.717338
1265.686168	179850.689963	35.722356
1266.815975	180176.472797	35.727373
1268.115916	180527.447968	35.732391
1269.179533	180865.353994	35.737408
1270.753782	181206.541310	35.742426
1272.124979	181564.251207	35.747444
1273.180605	181899.005075	35.752461
1274.480392	182242.072199	35.757479
1275.565847	182603.187150	35.762496
1277.274747	182939.058343	35.767514
1278.241777	183298.090722	35.772532
1279.865788	183652.206685	35.777549
1281.337244	183994.901557	35.782567
1282.632576	184330.494475	35.787584
1284.144835	184682.097229	35.792602
1285.294053	185034.130298	35.797620
1286.810375	185372.993380	35.802637
1288.320139	185731.622532	35.807655
1289.414735	186070.305717	35.812672
1290.807592	186409.436804	35.817690
1291.754290	186777.330150	35.822708
1293.062381	187125.415623	35.827725
1294.661773	187477.275893	35.832743
1295.486359	187828.288873	35.837760
1296.853214	188183.644578	35.842778
1298.238485	188549.662079	35.847796
1299.340028	188903.669820	35.852813
1300.643713	189267.788685	35.857831
1302.006750	189643.159480	35.862848
1303.703327	189979.837505	35.867866
1304.592892	190339.157069	35.872884
1306.280005	190701.076447	35.877901
1307.575268	191055.192397	35.882919
1309.046654	191418.954392	35.887936
1310.519877	191785.181021	35.892954
1311.641748	192148.421262	35.897972
1313.205048	192491.597150	35.902989
1314.901760	192861.601847	35.908007
1316.091148	193218.261693	35.913024
1317.246614	193569.140482	35.918042
1318.326575	193936.803486	35.923060
1319.546235	194298.250585	35.928077
1320.694593	194647.968821	35.933095
1321.816361	195022.194670	35.938112
1323.590030	195393.255681	35.943130
1324.603703	195754.237471	35.948148
1325.725956	196111.179047	35.953165
1326.929829	196493.639300	35.958183
1328.394729	196862.893729	35.963200
1329.823875	197228.703047	35.968218
1331.246897	197616.999126	35.973236
1332.533336	197985.705468	35.978253
1333.743473	198339.356804	35.983271
1334.956030	198703.267760	35.988288
1336.390620	199054.867298	35.993306
1337.341501	199420.094968	35.998324
1338.626686	199767.520623	36.003341
1340.039343	200148.431657	36.008359
1340.798746	200515.385461	36.013376
1342.591472	200875.441786	36.018394
1344.054689	201250.726303	36.023412
1345.384619	201611.662741	36.028429
1346.926481	201982.050220	36.033447
1347.974091	202349.791525	36.038464
1349.370810	202713.274632	36.043482
1350.412293	203098.453068	36.048500
1351.467623	203475.086526	36.053517
1353.167274	203855.386536	36.058535
1354.456440	204244.618601	36.063552
1355.840459	204626.244442	36.068570
1357.098459	205020.361372	36.073588
1358.373903	205409.055966	36.078605
1359.958927	205801.561394	36.083623
1361.153270	206193.206487	36.088640
1362.946413	206583.193063	36.093658
1363.879260	206989.004637	36.098676
1365.478498	207369.161565	36.103693
1366.740562	207774.034179	36.108711
1367.538804	208180.953556	36.113728
1369.420887	208593.244971	36.118746
1370.682268	208997.844730	36.123764
1371.993818	209397.257678	36.128781
1373.277770	209810.682667	36.133799
1374.511408	210226.898887	36.138816
1375.868017	210638.157526	36.143834
1377.401736	211055.522059	36.148852
1379.043620	211461.023734	36.153869
1380.647976	211871.181036	36.158887
1381.891277	212289.272702	36.163904
1383.728500	212705.541487	36.168922
1385.070055	213115.951386	36.173940
1386.449833	213533.975857	36.178957
1387.938836	213950.638306	36.183975
1389.222757	214354.181135	36.188992
1390.581664	214767.745153	36.194010
1392.207864	215179.844760	36.199028
1393.379569	215593.748261	36.204045
1395.110156	216023.155242	36.209063
1396.034070	216433.395482	36.214080
1397.329181	216845.887445	36.219098
1399.147114	217278.155755	36.224116
1400.682527	217695.462720	36.229133
1402.099241	218106.441693	36.234151
1403.575929	218535.521145	36.239168
1404.809182	218948.108648	36.244186
1406.403642	219353.831621	36.249204
1407.842849	219791.354905	36.254221
1409.286428	220258.112735	36.259239
1410.694115	220671.008786	36.264256
1412.287822	221093.908189	36.269274
1413.460559	221498.210880	36.274292
1415.235859	221915.292806	36.279309
1416.721043	222319.140727	36.284327
1417.839206	222744.715948	36.289344
1419.321215	223144.833884	36.294362
1420.990620	223558.841030	36.299380
1422.683230	223974.039665	36.304397
1424.664984	224374.130406	36.309415
1425.314544	224790.139182	36.314432
1426.957725	225181.729094	36.319450
1428.452557	225584.012600	36.324468
1429.696960	225965.333390	36.329485
1431.490045	226345.498088	36.334503
1432.865288	226750.497685	36.339520
1434.182619	227134.959759	36.344538
1435.134856	227513.488925	36.349556
1436.557635	227907.486383	36.354573
1437.998181	228292.769942	36.359591
1439.326870	228690.595397	36.364608
1440.783392	229098.662680	36.369626
1442.425992	229487.218530	36.374644
1443.499762	229889.839600	36.379661
1445.048585	230287.379614	36.384679
1446.084673	230713.377786	36.389696
1447.964397	231109.697190	36.394714
1449.166086	231517.585320	36.399732
1450.454470	231937.170072	36.404749
1452.344268	232344.286625	36.409767
1453.038568	232766.943742	36.414784
1454.723238	233190.149878	36.419802
1456.583805	233604.514039	36.424820
1457.885721	234029.436780	36.429837
1459.187134	234453.090725	36.434855
1460.785685	234892.420155	36.439872
1462.056141	235310.823470	36.444890
1463.531975	235749.261066	36.449908
1464.878429	236184.723817	36.454925
1466.222207	236612.694704	36.459943
1467.198279	237059.092685	36.464960
1468.963403	237505.336210	36.469978
1470.287591	237946.903512	36.474996
1471.457800	238390.504049	36.480013
1473.118034	238857.673896	36.485031
1474.729593	239318.477070	36.490048
1476.079398	239763.549942	36.495066
1477.495056	240234.827831	36.500084
1478.795400	240690.046356	36.505101
1480.491356	241140.958462	36.510119
1481.862483	241614.558480	36.515136
1483.647099	242075.872844	36.520154
1485.450848	242545.313752	36.525172
1486.949128	243010.411444	36.530189
1488.435584	243461.642323	36.535207
1490.079202	243923.898187	36.540224
1491.826913	244388.805013	36.545242
1493.517977	244848.184300	36.550260
1494.928197	245307.737764	36.555277
1496.310953	245760.437850	36.560295
1498.035593	246225.758197	36.565312
1499.285170	246684.095754	36.570330
1500.890961	247146.973148	36.575348
1502.188756	247619.986979	36.580365
1504.029769	248070.277985	36.585383
1505.242248	248547.270115	36.590400
1506.420238	249004.682991	36.595418
1508.128509	249479.536977	36.600436
1509.403078	249953.167598	36.605453
1510.883235	250428.187454	36.610471
1512.195998	250899.450451	36.615488
1513.826084	251383.134512	36.620506
1515.493520	251862.900873	36.625524
1517.178281	252340.276985	36.630541
1518.261788	252828.269666	36.635559
1519.859145	253303.324029	36.640576
1520.878715	253777.407209	36.645594
1522.777162	254265.647739	36.650612
1524.391635	254764.782670	36.655629
1525.822718	255230.466787	36.660647
1527.311962	255722.179909	36.665664
1528.755163	256180.724288	36.670682
1530.440428	256642.709204	36.675700
1531.723172	257130.240230	36.680717
1533.371698	257594.898964	36.685735
1534.701199	258063.598822	36.690752
1536.056626	258543.040137	36.695770
1537.483743	259018.074976	36.700788
1538.833903	259493.529059	36.705805
1540.293456	259988.220867	36.710823
1541.846106	260477.384840	36.715840
1543.637333	260971.234477	36.720858
1545.148646	261466.222628	36.725876
1546.313450	261963.960660	36.730893
1547.906266	262451.898530	36.735911
1549.660433	262965.314582	36.740928
1550.961365	263460.438699	36.745946
1553.076424	263948.289999	36.750964
1554.356494	264469.785794	36.755981
1556.164190	264954.486580	36.760999
1558.163091	265453.127355	36.766016
1559.545289	265962.386535	36.771034
1561.559371	266458.001211	36.776052
1562.792596	266968.173396	36.781069
1564.424157	267464.231506	36.786087
1566.221534	267964.326354	36.791104
1567.651992	268474.388518	36.796122
1569.464602	268971.685585	36.801140
1570.795471	269482.423655	36.806157
1572.516496	269976.406993	36.811175
1574.066288	270483.627598	36.816192
1575.507364	271006.920210	36.821210
1577.465061	271497.661926	36.826228
1579.418847	272010.554992	36.831245
1581.106110	272505.429863	36.836263
1582.716139	273004.838477	36.841280
1583.741713	273519.838483	36.846298
1585.531663	274028.640280	36.851316
1586.857881	274538.991105	36.856333
1588.463588	275059.456004	36.861351
1590.396534	275576.004760	36.866368
1591.666607	276086.209664	36.871386
1593.525011	276606.096490	36.876404
1595.026470	277128.073357	36.881421
1596.530459	277642.478792	36.886439
1597.891821	278157.135286	36.891456
1599.695418	278680.811709	36.896474
1601.452073	279212.699598	36.901492
1602.715380	279728.029176	36.906509
1604.477676	280254.756948	36.911527
1606.403494	280777.849322	36.916544
1607.229433	281319.639877	36.921562
1608.958534	281826.860333	36.926580
1610.563554	282356.428164	36.931597
1612.575104	282891.541230	36.936615
1614.144499	283427.716360	36.941632
1615.759111	283961.367672	36.946650
1617.369598	284484.425597	36.951668
1618.884285	285016.312049	36.956685
1620.755436	285554.386749	36.961703
1622.660303	286085.849786	36.966720
1624.122079	286609.738406	36.971738
1626.018233	287140.411928	36.976756
1627.460242	287674.282887	36.981773
1629.016738	288194.924578	36.986791
1630.575528	288721.253863	36.991808
1632.178307	289264.465509	36.996826
1633.891698	289792.949851	37.001844
1635.349533	290322.388790	37.006861
1637.209914	290832.277108	37.011879
1638.561056	291337.523055	37.016896
1639.810114	291866.457008	37.021914
1641.421068	292377.548986	37.026932
1643.013926	292901.265771	37.031949
1644.567892	293420.135415	37.036967
1646.250746	293949.344790	37.041984
1648.112896	294474.153546	37.047002
1649.699108	294988.210698	37.052020
1651.375296	295528.386922	37.057037
1652.893415	296054.134465	37.062055
1654.250298	296596.568168	37.067072
1655.869243	297133.215834	37.072090
1657.487558	297668.895873	37.077108
1659.007174	298225.442131	37.082125
1660.419027	298774.409081	37.087143
1662.435669	299332.645555	37.092160
1663.789031	299884.969060	37.097178
1665.576999	300441.891245	37.102196
1666.933389	300995.503647	37.107213
1668.801547	301568.534357	37.112231
1670.764462	302131.386957	37.117248
1672.274477	302711.454604	37.122266
1674.288171	303263.904607	37.127284
1675.956812	303843.253553	37.132301
1677.302728	304399.819957	37.137319
1679.092811	304983.865759	37.142336
1680.354516	305568.985522	37.147354
1682.232983	306137.618774	37.152372
1683.860267	306727.115194	37.157389
1685.440283	307320.551965	37.162407
1687.391018	307903.257073	37.167424
1688.864057	308501.046234	37.172442
1690.803066	309095.071914	37.177460
1692.693078	309685.673056	37.182477
1694.190512	310280.626654	37.187495
1695.862659	310879.051710	37.192512
1697.338242	311472.298761	37.197530
1698.837723	312064.140764	37.202548
1700.743060	312680.265138	37.207565
1702.888742	313287.202931	37.212583
1704.968881	313872.409081	37.217600
1706.445389	314494.506741	37.222618
1708.044899	315089.280336	37.227636
1709.736310	315687.436845	37.232653
1711.417883	316294.046268	37.237671
1713.409761	316894.835165	37.242688
1714.932945	317496.102712	37.247706
1716.636947	318108.432177	37.252724
1718.308750	318732.670933	37.257741
1719.924454	319339.316316	37.262759
1721.374648	319950.528963	37.267776
1723.164466	320573.766838	37.272794
1725.197422	321190.103084	37.277812
1726.859457	321814.772592	37.282829
1728.933044	322424.971401	37.287847
1730.652552	323035.426126	37.292864
1731.982171	323657.974818	37.297882
1734.207970	324267.775876	37.302900
1735.920864	324891.468200	37.307917
1736.888533	325509.005956	37.312935
1739.260274	326121.431146	37.317952
1741.008257	326744.464590	37.322970
1742.941844	327366.369388	37.327988
1744.884534	327981.258937	37.333005
1746.497553	328602.366166	37.338023
1748.498231	329206.265636	37.343040
1750.021884	329815.924698	37.348058
1751.977085	330411.339655	37.353076
1753.835816	330998.538775	37.358093
1755.403284	331578.112920	37.363111
1756.842314	332160.926628	37.368128
1758.592728	332768.080102	37.373146
1760.123104	333365.007059	37.378164
1761.769469	333967.950559	37.383181
1763.059335	334563.152731	37.388199
1765.018055	335172.048185	37.393216
1766.527430	335787.941324	37.398234
1768.414162	336405.288364	37.403252
1770.447568	337021.004870	37.408269
1771.558355	337665.754519	37.413287
1773.651324	338274.110472	37.418304
1775.377327	338898.740505	37.423322
1776.838024	339537.748789	37.428340
1778.848883	340174.653118	37.433357
1780.390036	340803.783570	37.438375
1782.182657	341443.779484	37.443392
1784.019183	342090.105733	37.448410
1786.277641	342728.003236	37.453428
1788.161955	343375.193353	37.458445
1790.019276	344014.257278	37.463463
1791.795103	344658.580259	37.468480
1793.512442	345317.371553	37.473498
1795.320991	345954.006812	37.478516
1797.238966	346611.452844	37.483533
1799.164320	347247.036350	37.488551
1801.111894	347884.967932	37.493568
1802.765262	348556.287794	37.498586
1804.636152	349212.385448	37.503604
1807.030471	349852.855709	37.508621
1808.652259	350521.258998	37.513639
1810.425870	351162.980638	37.518656
1812.211339	351821.008930	37.523674
1813.685466	352489.965696	37.528692
1815.256487	353141.107306	37.533709
1816.852549	353809.465735	37.538727
1819.427676	354484.072583	37.543744
1820.885669	355151.925708	37.548762
1822.563635	355819.021712	37.553780
1824.788937	356487.666410	37.558797
1826.346240	357170.544331	37.563815
1828.070740	357835.165121	37.568832
1829.657465	358511.723697	37.573850
1831.478057	359192.673019	37.578868
1833.392985	359879.228326	37.583885
1835.167559	360574.168181	37.588903
1836.765486	361269.150715	37.593920
1838.456483	361960.122666	37.598938
1840.311147	362660.798225	37.603956
1842.602828	363356.645121	37.608973
1843.864377	364078.045216	37.613991
1846.111325	364766.263670	37.619008
1847.889804	365463.198200	37.624026
1849.526654	366168.286972	37.629044
1851.681928	366870.639063	37.634061
1853.067328	367587.311262	37.639079
1854.977232	368295.715196	37.644096
1856.808339	369011.094759	37.649114
1858.705671	369719.879906	37.654132
1860.684828	370433.051777	37.659149
1862.461007	371148.729238	37.664167
1864.436083	371870.193931	37.669184
1866.361073	372593.935476	37.674202
1867.936984	373297.555921	37.679220
1869.858729	374021.700715	37.684237
1871.795598	374745.245079	37.689255
1873.779947	375431.027739	37.694272
1875.966840	376121.861481	37.699290
1876.923958	376819.985735	37.704308
1879.391578	377509.452489	37.709325
1880.953182	378218.962948	37.714343
1882.637855	378923.265171	37.719360
1884.444680	379619.519292	37.724378
1886.421142	380329.830779	37.729396
1888.194862	381042.924934	37.734413
1889.680145	381764.242187	37.739431
1891.713567	382474.321746	37.744448
1893.550163	383205.363284	37.749466
1895.333859	383934.977525	37.754484
1897.261425	384658.720147	37.759501
1899.227741	385405.462731	37.764519
1901.224201	386132.204006	37.769536
1902.783023	386874.264183	37.774554
1904.650207	387631.088060	37.779572
1906.777247	388366.352189	37.784589
1908.589797	389122.845527	37.789607
1910.627921	389870.588061	37.794624
1912.549620	390629.258249	37.799642
1914.275968	391399.552664	37.804660
1916.136915	392155.128421	37.809677
1918.236246	392932.116964	37.814695
1920.296217	393699.307932	37.819712
1922.327702	394455.635553	37.824730
1924.076168	395236.628352	37.829748
1926.326163	396001.778162	37.834765
1927.789782	396768.508248	37.839783
1929.586329	397546.112825	37.844800
1931.879702	398344.169408	37.849818
1933.779190	399126.201490	37.854836
1936.223793	399897.681509	37.859853
1937.949598	400684.997312	37.864871
1940.017798	401455.813894	37.869888
1941.892722	402240.553989	37.874906
1944.250117	403032.769812	37.879924
1946.340041	403803.849208	37.884941
1947.852389	404604.269365	37.889959
1949.700681	405383.378038	37.894976
1951.937444	406190.931020	37.899994
1953.617142	406973.874551	37.905012
1955.540150	407761.493724	37.910029
1957.831391	408571.274097	37.915047
1959.699330	409372.765355	37.920064
1961.411055	410168.229426	37.925082
1963.167201	410987.577288	37.930100
1965.297775	411782.747561	37.935117
1966.727759	412584.190759	37.940135
1969.042338	413389.618288	37.945152
1971.505706	414207.687210	37.950170
1973.105644	415019.312974	37.955188
1975.364950	415832.856557	37.960205
1977.449397	416631.232433	37.965223
1978.873435	417454.361110	37.970240
1981.098066	418267.479756	37.975258
1983.068491	419097.228020	37.980276
1985.262317	419905.462789	37.985293
1987.396022	420742.272206	37.990311
1989.375354	421557.149949	37.995328
1991.218211	422353.412230	38.000346
1992.787031	423181.852325	38.005364
1995.371096	423998.981883	38.010381
1996.849261	424817.659527	38.015399
1999.002284	425644.174129	38.020416
2000.907917	426477.183104	38.025434
2002.695685	427301.474144	38.030452
2004.752376	428093.136454	38.035469
2006.743641	428903.466341	38.040487
2008.526114	429703.778928	38.045504
2010.576312	430493.642108	38.050522
2012.738878	431311.810865	38.055540
2014.853003	432120.087827	38.060557
2016.579052	432927.338107	38.065575
2018.693024	433742.494713	38.070592
2020.594457	434564.997673	38.075610
2022.339636	435375.703712	38.080628
2024.183728	436192.945043	38.085645
2026.291473	437036.078450	38.090663
2028.274932	437866.548633	38.095680
2030.385533	438691.653710	38.100698
2032.439312	439541.282869	38.105716
2034.513773	440378.933838	38.110733
2036.483545	441221.631317	38.115751
2038.384440	442072.455387	38.120768
2040.616837	442913.780801	38.125786
2042.572326	443774.802612	38.130804
2045.018581	444623.971718	38.135821
2046.997853	445472.577951	38.140839
2048.963152	446339.822065	38.145856
2051.139723	447188.885638	38.150874
2053.149533	448057.622224	38.155892
2055.401045	448911.361163	38.160909
2057.701838	449782.104857	38.165927
2059.183997	450643.843396	38.170944
2061.643609	451506.650379	38.175962
2063.521594	452395.161072	38.180980
2065.588521	453275.359384	38.185997
2067.696389	454150.861304	38.191015
2069.539652	455040.429029	38.196032
2071.924121	455925.874516	38.201050
2073.388571	456817.653614	38.206068
2075.485072	457719.807386	38.211085
2077.458701	458601.918992	38.216103
2079.635797	459505.851589	38.221120
2082.252528	460406.435781	38.226138
2083.789573	461313.275203	38.231156
2086.085153	462211.506278	38.236173
2088.578261	463122.251810	38.241191
2090.241500	464045.123287	38.246208
2092.474416	464934.901570	38.251226
2094.519671	465856.564246	38.256244
2096.934794	466764.931339	38.261261
2099.155214	467673.995993	38.266279
2101.352294	468585.195243	38.271296
2104.070960	469485.501804	38.276314
2105.988336	470407.930756	38.281332
2107.497451	471313.000494	38.286349
2109.876496	472214.852380	38.291367
2111.543563	473131.128238	38.296384
2114.063725	474053.736676	38.301402
2115.769236	474980.071912	38.306420
2117.936375	475897.596384	38.311437
2120.069169	476831.094993	38.316455
2122.437233	477770.822218	38.321472
2124.555914	478679.681250	38.326490
2126.499121	479601.252549	38.331508
2128.712255	480536.521173	38.336525
2131.096794	481455.350968	38.341543
2132.949232	482388.210820	38.346560
2134.796405	483316.327417	38.351578
2136.851132	484263.752269	38.356596
2138.976192	485197.381837	38.361613
2141.101420	486139.142139	38.366631
2142.958927	487077.918236	38.371648
2145.131479	488013.563807	38.376666
2147.284179	488941.035704	38.381684
2149.179583	489851.086020	38.386701
2151.232386	490769.089010	38.391719
2153.211229	491705.680858	38.396736
2155.261634	492621.366047	38.401754
2157.301178	493557.444408	38.406772
2159.144435	494514.346725	38.411789
2161.321933	495445.152418	38.416807
2163.353857	496387.285085	38.421824
2165.800143	497347.108825	38.426842
2167.689851	498311.864221	38.431860
2170.315477	499258.482576	38.436877
2172.567281	500214.543311	38.441895
2174.598615	501187.787950	38.446912
2176.834418	502143.236814	38.451930
2178.790417	503122.484612	38.456948
2180.900773	504087.425939	38.461965
2183.112897	505070.853784	38.466983
2185.131175	506066.761635	38.472000
2187.163468	507054.185181	38.477018
2189.172059	508049.116562	38.482036
2191.305093	509044.924489	38.487053
2193.949190	510055.561118	38.492071
2195.956428	511060.088674	38.497088
2198.353542	512059.145347	38.502106
2200.364043	513081.895483	38.507124
2202.405930	514104.373064	38.512141
2204.723911	515111.618392	38.517159
2206.558517	516139.290782	38.522176
2209.336106	517163.867893	38.527194
2211.081413	518213.744365	38.532212
2213.300543	519242.610868	38.537229
2215.999478	520268.206097	38.542247
2218.168200	521324.100489	38.547264
2220.088575	522370.492128	38.552282
2222.677381	523419.875742	38.557300
2224.679220	524453.114536	38.562317
2226.879935	525511.585678	38.567335
2229.065633	526580.259713	38.572352
2231.675590	527624.513791	38.577370
2234.065769	528674.925463	38.582388
2236.099311	529747.880867	38.587405
2238.485873	530793.158866	38.592423
2240.716150	531854.248291	38.597440
2242.829580	532906.974031	38.602458
2245.272267	533980.511522	38.607476
2247.985614	535033.841521	38.612493
2250.910282	536090.483210	38.617511
2252.780503	537139.974516	38.622528
2255.595669	538194.769681	38.627546
2257.882710	539237.346554	38.632564
2260.116384	540284.485758	38.637581
2262.420168	541328.366915	38.642599
2264.718233	542387.617851	38.647616
2267.307280	543421.236160	38.652634
2269.465604	544464.709305	38.657652
2272.011090	545514.328699	38.662669
2274.328922	546541.173423	38.667687
2276.367946	547590.368567	38.672704
2278.628315	548628.686463	38.677722
2280.990733	549660.674509	38.682740
2283.137578	550715.146709	38.687757
2285.545788	551755.568356	38.692775
2287.348453	552806.869830	38.697792
2289.565923	553848.219530	38.702810
2292.086571	554896.175079	38.707828
2293.884573	555933.513356	38.712845
2296.451224	556955.769012	38.717863
2298.540528	557999.484015	38.722880
2300.562783	559008.908734	38.727898
2302.813115	560036.308133	38.732916
2305.084223	561074.376603	38.737933
2307.042086	562095.284265	38.742951
2309.164155	563139.997481	38.747968
2311.398166	564178.631958	38.752986
2313.456267	565243.029467	38.758004
2315.353089	566306.965120	38.763021
2317.406463	567363.104708	38.768039
2319.950481	568439.062546	38.773056
2322.496687	569536.068692	38.778074
2324.755686	570607.173026	38.783092
2326.865220	571693.574139	38.788109
2329.362210	572774.899774	38.793127
2331.576229	573880.373057	38.798144
2333.788201	574979.627438	38.803162
2335.846061	576089.550978	38.808180
2338.062867	577210.590676	38.813197
2340.683545	578322.131146	38.818215
2342.504345	579467.669919	38.823232
2344.773423	580580.622460	38.828250
2347.375064	581713.635296	38.833268
2349.583227	582869.982066	38.838285
2351.936202	584008.542998	38.843303
2354.087941	585169.898512	38.848320
2356.472113	586327.394849	38.853338
2359.179988	587485.880958	38.858356
2361.299215	588651.221654	38.863373
2363.839068	589818.686526	38.868391
2366.533587	590988.769455	38.873408
2368.521669	592164.568156	38.878426
2371.188285	593343.095979	38.883444
2373.497413	594523.369953	38.888461
2375.941014	595686.018318	38.893479
2378.640147	596869.300889	38.898496
2381.062565	598054.012920	38.903514
2383.838378	599245.659504	38.908532
2385.608338	600422.425668	38.913549
2388.471914	601599.643759	38.918567
2390.330533	602812.559761	38.923584
2392.891587	603992.788970	38.928602
2395.397885	605180.765974	38.933620
2397.332553	606393.792740	38.938637
2399.526449	607602.944179	38.943655
2402.452855	608811.496098	38.948672
2404.938887	610005.730109	38.953690
2407.564794	611221.980668	38.958708
2409.886972	612440.501309	38.963725
2412.091597	613653.706363	38.968743
2414.758550	614863.902396	38.973760
2417.285100	616083.492665	38.978778
2419.368464	617290.669810	38.983796
2421.739626	618501.767906	38.988813
2424.185035	619725.169926	38.993831
2426.847924	620945.850084	38.998848
2429.219256	622179.938268	39.003866
2431.804634	623403.555336	39.008884
2434.051667	624630.138669	39.013901
2436.736998	625841.469848	39.018919
2439.028785	627076.212600	39.023936
2441.949030	628288.828174	39.028954
2444.589231	629502.401414	39.033972
2446.987914	630732.408570	39.038989
2449.513044	631939.229740	39.044007
2451.806912	633163.129055	39.049024
2454.343320	634375.712118	39.054042
2456.888107	635559.647515	39.059060
2459.005096	636744.767521	39.064077
2461.159127	637921.461401	39.069095
2464.291476	639115.727454	39.074112
2466.485562	640295.239893	39.079130
2469.004348	641467.628697	39.084148
2470.979360	642671.204430	39.089165
2473.672590	643874.171411	39.094183
2475.502716	645059.382680	39.099200
2478.030956	646260.699024	39.104218
2480.457112	647477.099197	39.109236
2482.471408	648702.345991	39.114253
2484.687257	649931.448900	39.119271
2486.853407	651155.225570	39.124288
2489.576986	652407.918134	39.129306
2492.022884	653651.678445	39.134324
2494.364544	654919.766432	39.139341
2496.906130	656170.719614	39.144359
2499.257631	657451.933573	39.149376
2501.397224	658717.375508	39.154394
2504.224784	660008.836882	39.159412
2506.198348	661298.127153	39.164429
2508.630596	662580.648710	39.169447
2511.163785	663884.540349	39.174464
2513.709931	665195.471677	39.179482
2516.676702	666491.722140	39.184500
2518.820391	667817.144182	39.189517
2521.475060	669137.024311	39.194535
2524.111820	670464.037826	39.199552
2526.555484	671781.745288	39.204570
2529.390524	673109.201643	39.209588
2531.822981	674440.018557	39.214605
2534.201335	675788.704768	39.219623
2536.882493	677113.433369	39.224640
2539.695080	678452.615842	39.229658
2542.463030	679784.157912	39.234676
2545.075005	681141.225433	39.239693
2547.594565	682488.618937	39.244711
2550.241077	683817.214718	39.249728
2552.779589	685164.610061	39.254746
2555.447057	686510.444601	39.259764
2557.773989	687877.538108	39.264781
2560.673378	689228.195588	39.269799
2562.871223	690584.823178	39.274816
2564.972856	691949.650488	39.279834
2568.066157	693314.851323	39.284852
2570.331903	694682.014623	39.289869
2572.782002	696057.570209	39.294887
2575.732782	697430.846218	39.299904
2578.356551	698803.863946	39.304922
2581.136217	700189.832617	39.309940
2583.837738	701561.019265	39.314957
2585.886756	702940.228692	39.319975
2588.525354	704322.939555	39.324992
2591.179862	705716.181760	39.330010
2593.806111	707089.583666	39.335028
2596.710004	708484.965125	39.340045
2599.065797	709874.762250	39.345063
2601.637235	711255.929157	39.350080
2604.166067	712653.418429	39.355098
2607.175361	714033.370532	39.360116
2609.537751	715434.292024	39.365133
2612.294086	716820.168154	39.370151
2615.183194	718214.850187	39.375168
2617.482239	719602.867294	39.380186
2620.644337	720996.596644	39.385204
2623.319366	722395.465670	39.390221
2625.728558	723758.143207	39.395239
2628.372913	725115.119362	39.400256
2630.880247	726471.203211	39.405274
2633.371484	727809.915487	39.410292
2635.953167	729161.885814	39.415309
2638.659200	730511.438251	39.420327
2641.414500	731863.822212	39.425344
2643.361196	733237.304397	39.430362
2646.112321	734589.383097	39.435380
2648.610361	735958.559154	39.440397
2650.842747	737330.113328	39.445415
2653.787955	738713.853085	39.450432
2656.420229	740113.049425	39.455450
2659.120053	741494.521699	39.460468
2661.593654	742887.236607	39.465485
2663.949388	744283.080165	39.470503
2666.567840	745693.379298	39.475520
2668.991085	747110.903269	39.480538
2671.821336	748526.772842	39.485556
2674.271633	749960.932201	39.490573
2676.929807	751388.830274	39.495591
2679.900143	752825.283145	39.500608
2682.021186	754280.082672	39.505626
2684.980791	755716.295162	39.510644
2687.538702	757173.184826	39.515661
2690.190962	758642.188885	39.520679
2693.079282	760109.985283	39.525696
2695.415770	761583.298391	39.530714
2698.176231	763059.060065	39.535732
2700.775257	764534.314126	39.540749
2703.636462	766036.485200	39.545767
2706.076113	767524.754006	39.550784
2708.920938	769018.363230	39.555802
2711.781997	770517.028556	39.560820
2714.758560	772022.253027	39.565837
2717.234765	773532.953750	39.570855
2720.151947	775031.482063	39.575872
2722.800340	776540.211096	39.580890
2725.777335	778051.570832	39.585908
2728.408215	779579.907589	39.590925
2731.143150	781096.125630	39.595943
2733.901323	782616.685065	39.600960
2736.879320	784158.967757	39.605978
2739.743935	785673.664482	39.610996
2742.501991	787214.543137	39.616013
2745.094997	788737.268846	39.621031
2747.766047	790259.215308	39.626048
2750.591704	791794.582937	39.631066
2753.359350	793326.883150	39.636084
2756.170655	794881.624514	39.641101
2758.654591	796404.042895	39.646119
2761.703066	797951.795843	39.651136
2764.276561	799513.090611	39.656154
2767.349657	801053.492726	39.661172
2770.192052	802597.897381	39.666189
2772.822661	804140.035019	39.671207
2775.779699	805685.833826	39.676224
2778.279529	807243.341666	39.681242
2781.304735	808788.380961	39.686260
2784.313248	810341.627506	39.691277
2786.759034	811887.965608	39.696295
2789.866917	813446.936224	39.701312
2792.542112	814995.995253	39.706330
2795.926126	816531.932284	39.711348
2798.895553	818080.378449	39.716365
2801.447994	819624.629686	39.721383
2804.411668	821173.091770	39.726400
2806.953745	822715.065900	39.731418
2809.797511	824248.436189	39.736436
2812.662283	825758.378950	39.741453
2815.409030	827257.560401	39.746471
2818.454277	828771.851564	39.751488
2821.251884	830285.150492	39.756506
2823.828106	831785.758517	39.761524
2826.312664	833281.602145	39.766541
2828.919753	834795.732921	39.771559
2832.092136	836298.265317	39.776576
2834.689598	837816.800400	39.781594
2837.312547	839344.413300	39.786612
2839.996802	840860.460344	39.791629
2842.693262	842400.029065	39.796647
2845.637046	843931.451460	39.801664
2848.433701	845481.878730	39.806682
2851.498702	847024.006451	39.811700
2854.366661	848575.799596	39.816717
2857.025596	850133.462094	39.821735
2860.418126	851681.872659	39.826752
2862.533949	853253.903356	39.831770
2865.560186	854820.434424	39.836788
2868.305302	856404.088268	39.841805
2870.826362	857988.731363	39.846823
2873.848998	859582.682770	39.851840
2876.340258	861186.200931	39.856858
2879.046864	862791.590234	39.861876
2882.127397	864404.929022	39.866893
2884.537763	866025.218430	39.871911
2887.594331	867653.009654	39.876928
2890.706170	869275.024878	39.881946
2893.645044	870919.388283	39.886964
2896.463840	872554.219843	39.891981
2899.126542	874218.149401	39.896999
2902.180805	875867.616066	39.902016
2904.894431	877522.871104	39.907034
2908.021007	879181.172834	39.912052
2910.776858	880836.555396	39.917069
2913.100611	882516.478370	39.922087
2916.238414	884196.171673	39.927104
2919.017254	885889.060309	39.932122
2922.293021	887570.462261	39.937140
2925.275084	889256.541255	39.942157
2928.178015	890957.968651	39.947175
2930.989046	892646.944650	39.952192
2934.343643	894358.675350	39.957210
2937.134404	896054.558701	39.962228
2940.139144	897767.060358	39.967245
2943.237830	899470.646332	39.972263
2946.110745	901170.192280	39.977280
2948.883039	902881.859048	39.982298
2952.302614	904600.022621	39.987316
2955.389013	906314.634231	39.992333
2957.857887	908026.319425	39.997351
2960.901579	909733.055007	40.002368
2964.324809	911455.357689	40.007386
2967.194821	913167.986478	40.012404
2970.453114	914873.195878	40.017421
2973.094088	916576.056061	40.022439
2976.145428	918299.831765	40.027456
2979.573958	920011.575489	40.032474
2982.218368	921732.027439	40.037492
2985.463237	923440.704205	40.042509
2988.593402	925159.410249	40.047527
2991.436600	926870.423223	40.052544
2994.383108	928587.966916	40.057562
2997.062522	930306.057027	40.062580
3000.158335	932029.847166	40.067597
3003.157656	933754.913305	40.072615
3006.273604	935460.826000	40.077632
3009.428001	937139.192870	40.082650
3012.379647	938798.975581	40.087668
3015.139385	940467.637366	40.092685
3018.035785	942156.395834	40.097703
3021.133933	943812.841103	40.102720
3024.089243	945475.374451	40.107738
3026.380966	947163.655282	40.112756
3029.942770	948834.941720	40.117773
3032.563693	950537.340552	40.122791
3035.394833	952247.632243	40.127808
3038.677072	953941.155997	40.132826
3041.244621	955669.460201	40.137844
3044.309208	957429.178807	40.142861
3046.628362	959202.858804	40.147879
3049.716749	960991.508136	40.152896
3052.760602	962778.143821	40.157914
3055.543031	964589.767370	40.162932
3058.433928	966387.813066	40.167949
3061.340202	968212.143856	40.172967
3064.287643	970036.376571	40.177984
3067.050632	971886.404787	40.183002
3070.313108	973729.803921	40.188020
3073.448927	975583.357050	40.193037
3076.423023	977438.676246	40.198055
3079.142629	979306.785904	40.203072
3082.335739	981187.845119	40.208090
3085.089135	983075.953020	40.213108
3088.359938	984954.784083	40.218125
3090.830628	986857.846577	40.223143
3093.843642	988781.586736	40.228160
3097.031726	990688.212107	40.233178
3100.316927	992604.390209	40.238196
3102.873173	994533.551019	40.243213
3105.821587	996489.000240	40.248231
3109.360364	998434.451532	40.253248
3112.269540	1000391.377186	40.258266
3114.895411	1002354.854891	40.263284
3118.525114	1004325.441120	40.268301
3121.513534	1006312.127055	40.273319
3124.416840	1008285.330341	40.278336
3127.721908	1010271.054685	40.283354
3131.011770	1012264.026063	40.288372
3134.011105	1014253.627959	40.293389
3137.230693	1016259.625758	40.298407
3140.212775	1018254.494370	40.303424
3143.300048	1020265.276841	40.308442
3146.259011	1022287.641653	40.313460
3149.369764	1024297.650560	40.318477
3152.520914	1026313.019402	40.323495
3155.676564	1028323.024170	40.328512
3158.953238	1030364.057518	40.333530
3162.163537	1032393.157448	40.338548
3165.134012	1034425.322058	40.343565
3168.063730	1036463.697593	40.348583
3171.388401	1038503.286602	40.353600
3174.391992	1040550.181042	40.358618
3177.388222	1042605.765586	40.363636
3180.958903	1044640.748095	40.368653
3184.446251	1046699.261687	40.373671
3187.251780	1048741.048634	40.378688
3190.464968	1050795.485294	40.383706
3193.250916	1052857.115602	40.388724
3196.777987	1054912.758698	40.393741
3200.097018	1056961.999811	40.398759
3203.437089	1059028.056815	40.403776
3206.594786	1061097.978433	40.408794
3209.474711	1063159.295034	40.413812
3212.966544	1065195.554838	40.418829
3216.260318	1067221.978847	40.423847
3219.110263	1069236.316029	40.428864
3222.305294	1071252.060735	40.433882
3225.090423	1073264.543582	40.438900
3227.863184	1075275.042801	40.443917
3231.072604	1077317.956458	40.448935
3233.882614	1079345.909677	40.453952
3237.305861	1081388.316753	40.458970
3240.110815	1083444.406716	40.463988
3243.314723	1085503.765499	40.469005
3246.581127	1087572.846990	40.474023
3249.652962	1089630.950156	40.479040
3252.691788	1091707.282616	40.484058
3256.225405	1093812.809007	40.489076
3259.662931	1095911.616332	40.494093
3262.643721	1098009.875516	40.499111
3265.441478	1100120.032010	40.504128
3268.693570	1102234.054769	40.509146
3271.812155	1104371.947442	40.514164
3274.754611	1106520.068535	40.519181
3278.030987	1108673.370239	40.524199
3280.929596	1110832.818706	40.529216
3284.208055	1113004.463534	40.534234
3287.229086	1115184.685271	40.539252
3290.551274	1117377.086968	40.544269
3293.711002	1119571.373006	40.549287
3296.941216	1121772.439691	40.554304
3300.454953	1123979.862493	40.559322
3303.337799	1126202.702237	40.564340
3306.912820	1128420.612582	40.569357
3310.353022	1130648.714222	40.574375
3313.092591	1132890.592643	40.579392
3316.561900	1135140.120350	40.584410
3319.564034	1137396.820354	40.589428
3323.113794	1139650.955510	40.594445
3326.471175	1141916.083732	40.599463
3329.805156	1144182.610343	40.604480
3333.213507	1146446.167718	40.609498
3336.962858	1148719.753343	40.614516
3340.420848	1150988.345583	40.619533
3343.597257	1153273.283268	40.624551
3346.907591	1155548.808371	40.629568
3350.549088	1157821.595980	40.634586
3353.958122	1160101.829041	40.639604
3357.346350	1162376.267791	40.644621
3360.515879	1164665.957394	40.649639
3363.748229	1166945.407200	40.654656
3367.265538	1169240.004151	40.659674
3370.890733	1171534.045167	40.664692
3373.826063	1173829.353380	40.669709
3377.470356	1176122.217537	40.674727
3380.483772	1178415.302533	40.679744
3384.073243	1180706.153989	40.684762
3387.737529	1183015.600628	40.689780
3391.158776	1185324.621582	40.694797
3395.021317	1187625.975482	40.699815
3398.305415	1189921.713637	40.704832
3401.583231	1192214.746243	40.709850
3404.787121	1194516.887560	40.714868
3408.371733	1196811.853008	40.719885
3411.736410	1199122.862691	40.724903
3415.076704	1201417.498462	40.729920
3418.873621	1203709.070819	40.734938
3422.257377	1206017.163085	40.739956
3425.880223	1208316.797391	40.744973
3429.230915	1210599.011046	40.749991
3432.750931	1212895.950221	40.755008
3436.254773	1215160.445901	40.760013
3439.260432	1217392.766171	40.765018
3442.609159	1219549.299574	40.770023
3446.037571	1221652.320766	40.775028
3449.183096	1223684.308444	40.780032
3452.529350	1225615.121528	40.785037
3455.425271	1227485.192126	40.790042
3458.461189	1229269.215214	40.795047
3461.405992	1230979.438951	40.800052
3464.134445	1232601.791460	40.805056
3466.850139	1234150.671783	40.810061
3469.272234	1235624.982281	40.815066
3471.677052	1237011.705542	40.820071
3474.446073	1238337.103539	40.825076
3476.198515	1239596.146520	40.830080
3478.425803	1240771.796305	40.835085
3480.825064	1241888.162634	40.840090
3482.856606	1242943.048348	40.845095
3484.933462	1243916.244661	40.850100
3486.484617	1244827.138864	40.855104
3488.440138	1245704.522014	40.860109
3489.846241	1246504.141350	40.865114
3491.458616	1247250.071562	40.870119
3493.025899	1247954.085538	40.875124
3494.262876	1248597.109307	40.880128
3496.061134	1249196.297899	40.885133
3497.027567	1249762.392305	40.890138
3498.678698	1250266.177163	40.895143
3499.701090	1250730.175447	40.900148
3500.595902	1251180.687384	40.905152
3502.107198	1251573.768812	40.910157
3502.918128	1251919.398730	40.915162
3503.525335	1252231.430965	40.920167
3504.777802	1252512.795479	40.925172
3505.492074	1252777.152429	40.930176
3506.643038	1252996.032691	40.935181
3507.123587	1253200.255357	40.940186
3507.754730	1253361.192177	40.945191
3508.655266	1253510.570455	40.950196
3509.210862	1253635.127441	40.955200
3510.155431	1253724.999028	40.960205
3510.492300	1253788.611264	40.965210
3511.125237	1253837.881443	40.970215
3511.678165	1253881.410236	40.975220
3512.149756	1253887.179496	40.980224
3512.782753	1253878.444179	40.985229
3513.469051	1253852.437768	40.990234
3513.556640	1253805.183769	40.995239
3514.454608	1253737.934493	41.000244
3514.364712	1253673.260102	41.005248
3515.042343	1253571.054795	41.010253
3515.495781	1253472.132863	41.015258
3515.728111	1253370.832144	41.020263
3515.861047	1253236.873336	41.025268
3516.533035	1253095.117928	41.030272
3516.641242	1252938.413699	41.035277
3516.854251	1252776.396103	41.040282
3516.850038	1252604.476090	41.045287
3517.538826	1252416.654148	41.050292
3518.025353	1252230.622405	41.055296
3517.735105	1252033.942021	41.060301
3517.802862	1251820.389871	41.065306
3518.172633	1251607.057428	41.070311
3518.584354	1251395.287510	41.075316
3518.684356	1251157.095461	41.080320
3518.749947	1250923.262296	41.085325
3518.828920	1250678.643447	41.090330
3518.580451	1250416.699560	41.095335
3518.978117	1250166.338031	41.100340
3518.973068	1249924.018100	41.105344
3519.529870	1249662.923898	41.110349
3519.614292	1249391.397238	41.115354
3519.242996	1249109.062086	41.120359
3519.524200	1248840.445863	41.125364
3519.742527	1248572.197237	41.130368
3520.154526	1248273.613279	41.135373
3520.057602	1247991.820427	41.140378
3520.007677	1247707.866799	41.145383
3520.483051	1247391.471773	41.150388
3520.282100	1247100.074390	41.155392
3520.609183	1246796.305200	41.160397
3520.428033	1246496.505005	41.165402
3520.642204	1246169.759163	41.170407
3521.000937	1245861.559549	41.175412
3520.389468	1245542.252395	41.180416
3520.773487	1245214.393860	41.185421
3520.892218	1244898.737247	41.190426
3520.932134	1244578.145852	41.195431
3521.096940	1244247.656922	41.200436
3520.986280	1243922.213211	41.205440
3521.134463	1243586.475998	41.210445
3521.174248	1243256.593508	41.215450
3521.035527	1242915.092447	41.220455
3521.158656	1242566.920861	41.225460
3520.970270	1242239.148621	41.230464
3521.224483	1241891.001707	41.235469
3521.198408	1241554.227270	41.240474
3521.039493	1241203.402795	41.245479
3521.503943	1240871.154006	41.250484
3521.108100	1240528.509792	41.255488
3521.438491	1240171.949584	41.260493
3521.163919	1239829.144756	41.265498
3521.378061	1239479.534775	41.270503
3521.433886	1239117.826109	41.275508
3521.371606	1238777.334867	41.280512
3521.260253	1238405.828476	41.285517
3521.601984	1238063.826104	41.290522
3521.481942	1237706.793284	41.295527
3521.409962	1237349.913500	41.300532
3521.407060	1236993.742054	41.305536
3521.389441	1236632.053410	41.310541
3521.266096	1236271.846391	41.315546
3521.397055	1235920.978926	41.320551
3521.254851	1235557.277844	41.325556
3521.052494	1235193.094701	41.330560
3521.080178	1234835.741249	41.335565
3521.272277	1234475.354111	41.340570
3521.305715	1234122.700771	41.345575
3521.412611	1233757.897360	41.350580
3520.844616	1233402.217850	41.355584
3521.043436	1233050.301122	41.360589
3520.840360	1232696.375702	41.365594
3520.982641	1232324.100238	41.370599
3521.303896	1231976.469317	41.375604
3520.811185	1231620.279181	41.380608
3520.914053	1231247.837788	41.385613
3520.680697	1230892.019795	41.390618
3520.858508	1230529.395843	41.395623
3520.999421	1230161.157234	41.400628
3520.843374	1229819.424499	41.405632
3520.755421	1229445.856177	41.410637
3521.040394	1229096.914354	41.415642
3520.997043	1228729.721205	41.420647
3521.156189	1228362.654655	41.425652
3520.533217	1227999.981478	41.430656
3520.891210	1227615.663454	41.435661
3521.070985	1227267.079438	41.440666
3520.148214	1226907.083105	41.445671
3520.421278	1226542.478567	41.450676
3520.485662	1226187.120808	41.455680
3520.869591	1225818.806564	41.460685
3520.657328	1225467.363652	41.465690
3520.213995	1225108.373994	41.470695
3520.404827	1224748.601081	41.475700
3520.063366	1224402.799813	41.480704
3520.063878	1224038.527034	41.485709
3520.270038	1223683.997623	41.490714
3520.020843	1223323.075807	41.495719
3520.085092	1222957.781315	41.500724
3519.949030	1222614.252285	41.505728
3520.177004	1222251.868412	41.510733
3520.032118	1221907.639339	41.515738
3519.883102	1221544.146334	41.520743
3520.322554	1221193.140936	41.525748
3519.848455	1220840.206587	41.530752
3519.675397	1220484.675718	41.535757
3519.630318	1220139.749999	41.540762
3519.537460	1219797.518431	41.545767
3519.802253	1219435.301571	41.550772
3519.543641	1219086.695364	41.555776
3519.891009	1218742.357923	41.560781
3519.819256	1218391.056552	41.565786
3519.385805	1218033.808503	41.570791
3519.916249	1217667.309516	41.575796
3519.707427	1217324.743895	41.580800
3519.559652	1216969.524254	41.585805
3519.648581	1216614.614854	41.590810
3519.410681	1216268.991216	41.595815
3519.697700	1215915.964094	41.600820
3519.641688	1215576.154534	41.605824
3519.636853	1215219.667266	41.610829
3519.469554	1214866.548820	41.615834
3519.440962	1214514.973161	41.620839
3519.611062	1214153.238233	41.625844
3519.395984	1213810.998801	41.630848
3519.453774	1213454.190797	41.635853
3519.565540	1213108.201863	41.640858
3519.525738	1212752.670749	41.645863
3519.375954	1212403.776632	41.650868
3519.027945	1212058.447316	41.655872
3518.891520	1211712.217546	41.660877
3519.151220	1211363.278528	41.665882
3518.759418	1211015.920550	41.670887
3519.219662	1210676.916599	41.675892
3519.123864	1210342.755865	41.680896
3519.205198	1209991.505974	41.685901
3519.020957	1209640.182078	41.690906
3519.026051	1209290.581828	41.695911
3518.958273	1208951.269598	41.700916
3518.654638	1208606.448855	41.705920
3518.793863	1208263.030312	41.710925
3518.840293	1207921.477104	41.715930
3519.016040	1207585.218462	41.720935
3519.056518	1207240.904695	41.725940
3518.763801	1206889.035141	41.730944
3518.833912	1206534.833351	41.735949
3518.657719	1206192.264701	41.740954
3518.628201	1205862.391104	41.745959
3518.608423	1205507.289875	41.750964
3518.448518	1205176.362923	41.755968
3518.766792	1204827.999396	41.760973
3518.428914	1204484.031259	41.765978
3518.200501	1204151.549981	41.770983
3518.371357	1203812.232889	41.775988
3518.459396	1203484.530194	41.780992
3517.973273	1203138.434061	41.785997
3518.016263	1202811.914479	41.791002
3517.915552	1202469.178403	41.796007
3518.088481	1202132.937587	41.801012
3517.834073	1201799.276822	41.806016
3518.076982	1201474.795913	41.811021
3518.063020	1201150.805708	41.816026
3517.956463	1200821.839775	41.821031
3518.402800	1200480.662810	41.826036
3518.000192	1200143.823853	41.831040
3518.055493	1199818.612699	41.836045
3517.593331	1199485.304877	41.841050
3517.433747	1199156.522514	41.846055
3517.779877	1198818.629088	41.851060
3517.657924	1198505.466909	41.856064
3517.728234	1198165.042679	41.861069
3517.692365	1197835.967874	41.866074
3517.573352	1197511.484094	41.871079
3517.319328	1197191.976151	41.876084
3517.468355	1196868.721613	41.881088
3517.765512	1196524.866586	41.886093
3517.855644	1196199.233172	41.891098
3517.376509	1195881.839969	41.896103
3517.591695	1195551.920708	41.901108
3517.300678	1195229.574569	41.906112
3517.462707	1194897.744464	41.911117
3517.445759	1194571.744147	41.916122
3516.911456	1194258.767126	41.921127
3517.065811	1193917.296999	41.926132
3517.125299	1193610.286953	41.931136
3517.113815	1193291.060578	41.936141
3517.136716	1192970.775588	41.941146
3517.009156	1192653.689210	41.946151
3517.233585	1192321.870937	41.951156
3517.148621	1192015.823122	41.956160
3517.175472	1191692.827718	41.961165
3516.864118	1191366.297469	41.966170
3516.850259	1191065.067297	41.971175
3517.157275	1190744.879267	41.976180
3516.847433	1190430.129462	41.981184
3516.706095	1190095.315157	41.986189
3516.829189	1189790.416876	41.991194
3516.694552	1189470.316577	41.996199
3516.737891	1189155.712931	42.001204
3516.791377	1188845.694573	42.006208
3516.754950	1188525.331571	42.011213
3516.731239	1188207.296969	42.016218
3516.560704	1187901.019409	42.021223
3516.757296	1187583.568307	42.026228
3516.947501	1187269.577918	42.031232
3516.827451	1186954.209026	42.036237
3516.691074	1186627.914694	42.041242
3516.418784	1186324.005624	42.046247
3516.429194	1186005.641953	42.051252
3516.368848	1185709.092112	42.056256
3516.261431	1185383.090772	42.061261
3516.336855	1185086.294775	42.066266
3516.123138	1184771.184579	42.071271
3516.380340	1184464.633179	42.076276
3516.360907	1184151.899442	42.081280
3516.058222	1183843.992222	42.086285
3516.150379	1183536.566269	42.091290
3516.257756	1183243.705697	42.096295
3516.201097	1182918.670162	42.101300
3515.787525	1182631.225040	42.106304
3515.862193	1182326.741908	42.111309
3515.910500	1182021.303985	42.116314
3515.590246	1181715.814644	42.121319
3515.997166	1181414.706133	42.126324
3515.509130	1181124.271495	42.131328
3515.793991	1180830.774732	42.136333
3515.353410	1180524.387726	42.141338
3515.514237	1180225.792913	42.146343
3515.767570	1179938.842022	42.151348
3515.432845	1179651.030436	42.156352
3515.677814	1179337.491966	42.161357
3515.528482	1179045.566778	42.166362
3515.171358	1178752.434995	42.171367
3515.477955	1178454.467829	42.176372
3515.638634	1178170.166033	42.181376
3515.435994	1177868.387103	42.186381
3515.327678	1177566.009875	42.191386
3514.944245	1177282.973853	42.196391
3515.319641	1176989.056689	42.201396
3514.847950	1176697.429545	42.206400
3515.328459	1176417.973058	42.211405
3515.465278	1176120.748161	42.216410
3515.101520	1175831.787460	42.221415
3515.307316	1175539.324140	42.226420
3515.152027	1175240.400681	42.231424
3515.149325	1174954.347754	42.236429
3514.893354	1174668.603598	42.241434
3514.678424	1174377.275388	42.246439
3514.836776	1174088.320416	42.251444
3514.982254	1173808.401930	42.256448
3514.752848	1173518.725021	42.261453
3514.808402	1173236.339322	42.266458
3514.341324	1172973.071004	42.271463
3514.783766	1172683.236992	42.276468
3514.626139	1172402.255630	42.281472
3515.033427	1172129.370647	42.286477
3514.782439	1171837.717725	42.291482
3514.520944	1171556.424943	42.296487
3514.613814	1171267.229999	42.301492
3514.708020	1170983.206731	42.306496
3514.623761	1170696.084462	42.311501
3515.015328	1170420.188378	42.316506
3514.461622	1170138.018185	42.321511
3514.636974	1169848.825368	42.326516
3514.755940	1169585.195068	42.331520
3514.727409	1169299.024608	42.336525
3514.685744	1169003.310093	42.341530
3514.347648	1168729.143306	42.346535
3514.839136	1168444.161484	42.351540
3514.407390	1168166.960700	42.356544
3514.123765	1167889.437658	42.361549
3514.306711	1167597.570585	42.366554
3514.016224	1167325.209987	42.371559
3514.424807	1167054.608000	42.376564
3514.158111	1166779.571928	42.381568
3513.981328	1166503.090468	42.386573
3514.033657	1166233.448716	42.391578
3513.864549	1165979.691505	42.396583
3514.440516	1165697.567324	42.401588
3513.961315	1165432.409611	42.406592
3513.651205	1165153.801373	42.411597
3513.800698	1164887.757053	42.416602
3513.807080	1164623.611593	42.421607
3513.880402	1164356.513958	42.426612
3513.661456	1164105.318488	42.431616
3513.574193	1163825.374947	42.436621
3513.604848	1163558.149141	42.441626
3513.630183	1163298.656689	42.446631
3513.647924	1163032.350823	42.451636
3513.374572	1162781.478657	42.456640
3513.296957	1162513.745009	42.461645
3513.396173	1162250.598256	42.466650
3513.404849	1162001.626442	42.471655
3513.668091	1161740.222319	42.476660
3513.356088	1161464.819735	42.481664
3513.023159	1161196.588329	42.486669
3513.365005	1160942.691695	42.491674
3512.990672	1160690.412904	42.496679
3513.496503	1160430.793766	42.501684
3512.971771	1160170.197250	42.506688
3513.133546	1159926.111245	42.511693
3513.218369	1159672.668079	42.516698
3512.951939	1159414.260173	42.521703
3512.860328	1159169.046254	42.526708
3512.747644	1158925.337041	42.531712
3512.865344	1158664.938087	42.536717
3513.048127	1158414.538106	42.541722
3512.783060	1158169.116917	42.546727
3512.918646	1157916.620698	42.551732
3513.021489	1157666.954720	42.556736
3512.934644	1157414.849269	42.561741
3513.069441	1157167.802280	42.566746
3512.820381	1156927.900364	42.571751
3512.949514	1156657.374506	42.576756
3512.888729	1156414.202245	42.581760
3512.587173	1156156.680191	42.586765
3512.624207	1155907.603572	42.591770
3512.417370	1155661.960999	42.596775
3512.752447	1155419.623538	42.601780
3512.395298	1155178.618857	42.606784
3512.249234	1154939.366051	42.611789
3512.540613	1154690.284474	42.616794
3512.363936	1154450.635991	42.621799
3512.570970	1154204.384020	42.626804
3512.432609	1153969.817258	42.631808
3512.262183	1153719.062352	42.636813
3512.471741	1153476.182822	42.641818
3512.106689	1153236.036806	42.646823
3512.325157	1152999.285787	42.651828
3512.297208	1152764.268485	42.656832
3511.691852	1152519.869898	42.661837
3511.869225	1152290.098503	42.666842
3511.554338	1152057.368803	42.671847
3512.134837	1151823.629306	42.676852
3512.012228	1151591.699399	42.681856
3511.734813	1151351.263583	42.686861
3512.255600	1151119.017540	42.691866
3512.049129	1150899.001122	42.696871
3512.174207	1150650.323843	42.701876
3511.851840	1150425.003930	42.706880
3511.773868	1150190.542858	42.711885
3511.971719	1149958.204144	42.716890
3511.591386	1149725.192739	42.721895
3511.953907	1149489.680853	42.726900
3511.615086	1149259.199269	42.731904
3511.532420	1149032.833170	42.736909
3511.924504	1148801.927057	42.741914
3511.268539	1148574.688448	42.746919
3511.620454	1148345.758308	42.751924
3511.497655	1148129.496563	42.756928
3511.387351	1147896.265101	42.761933
3511.547403	1147676.053761	42.766938
3511.439629	1147444.223088	42.771943
3511.511146	1147222.396646	42.776948
3511.237003	1147003.839583	42.781952
3511.071998	1146778.906437	42.786957
3511.454945	1146558.896063	42.791962
3510.914223	1146346.136388	42.796967
3511.369508	1146130.360889	42.801972
3511.190172	1145910.131769	42.806977
3511.227086	1145672.038874	42.811981
3511.268109	1145454.218780	42.816986
3511.256814	1145237.156638	42.821991
3511.392284	1145007.738221	42.826996
3511.373502	1144797.768795	42.832001
3510.977096	1144578.657473	42.837005
3511.265072	1144357.623046	42.842010
3511.044114	1144143.868710	42.847015
3511.269218	1143915.051760	42.852020
3511.066945	1143706.681030	42.857025
3511.153806	1143491.048071	42.862029
3510.983987	1143267.198817	42.867034
3510.723508	1143063.932888	42.872039
3511.217523	1142835.593914	42.877044
3511.128207	1142627.162033	42.882049
3511.161048	1142412.252678	42.887053
3510.921860	1142197.663925	42.892058
3510.761647	1141979.544078	42.897063
3510.836125	1141766.972856	42.902068
3510.896171	1141564.165608	42.907073
3510.936717	1141340.200148	42.912077
3510.728708	1141116.645602	42.917082
3510.463894	1140917.661626	42.922087
3510.606637	1140691.944296	42.927092
3510.630726	1140497.166138	42.932097
3510.526643	1140297.373377	42.937101
3510.618680	1140079.133659	42.942106
3510.281059	1139868.451709	42.947111
3510.532357	1139657.189936	42.952116
3510.351306	1139463.451331	42.957121
3510.534421	1139257.688664	42.962125
3510.702303	1139055.052237	42.967130
3510.068081	1138852.160545	42.972135
3510.559249	1138635.978440	42.977140
3510.243689	1138437.668885	42.982145
3510.320894	1138239.287222	42.987149
3510.800879	1138026.309218	42.992154
3510.205743	1137816.537255	42.997159
3510.467463	1137619.905561	43.002164
3510.253056	1137417.174554	43.007169
3509.883861	1137212.467682	43.012173
3510.579723	1137006.058503	43.017178
3510.315025	1136815.084964	43.022183
3510.309906	1136614.187603	43.027188
3510.480960	1136403.473983	43.032193
3510.300756	1136201.260549	43.037197
3510.339861	1135999.762931	43.042202
3510.318340	1135808.997986	43.047207
3510.341894	1135591.154500	43.052212
3510.077873	1135403.738615	43.057217
3509.978915	1135204.037875	43.062221
3510.012501	1134995.855184	43.067226
3509.984980	1134806.004912	43.072231
3509.876224	1134600.869427	43.077236
3509.888205	1134407.104193	43.082241
3509.816827	1134203.561928	43.087245
3510.039323	1134005.187967	43.092250
3510.039601	1133822.612257	43.097255
3510.071633	1133627.580361	43.102260
3509.954925	1133427.625740	43.107265
3509.706582	1133232.815530	43.112269
3509.696982	1133046.889621	43.117274
3509.680543	1132849.081898	43.122279
3509.970276	1132654.161857	43.127284
3509.627805	1132462.949495	43.132289
3509.320745	1132266.498211	43.137293
3509.451944	1132080.515309	43.142298
3509.084642	1131896.508575	43.147303
3509.176392	1131714.035410	43.152308
3509.299002	1131527.654460	43.157313
3509.263099	1131344.619434	43.162317
3509.263081	1131166.419326	43.167322
3509.271495	1130987.546545	43.172327
3509.228812	1130807.915781	43.177332
3509.276578	1130619.139124	43.182337
3509.277968	1130432.264504	43.187341
3509.025334	1130250.178060	43.192346
3509.155413	1130080.285247	43.197351
3509.158443	1129896.813751	43.202356
3509.391068	1129714.819200	43.207361
3509.193454	1129532.128720	43.212365
3509.133904	1129346.652079	43.217370
3508.906326	1129176.979489	43.222375
3508.912668	1128996.994289	43.227380
3508.964452	1128803.113294	43.232385
3508.827139	1128638.638291	43.237389
3508.906018	1128460.619840	43.242394
3508.680990	1128288.065799	43.247399
3509.007601	1128119.694642	43.252404
3508.900931	1127944.447286	43.257409
3508.948141	1127766.981467	43.262413
3508.938956	1127580.103569	43.267418
3508.398626	1127423.741401	43.272423
3508.706273	1127251.066040	43.277428
3508.755939	1127083.944222	43.282433
3508.390652	1126896.244956	43.287437
3508.563277	1126728.616157	43.292442
3508.407438	1126572.260793	43.297447
3508.558709	1126398.061580	43.302452
3508.620259	1126244.990253	43.307457
3508.288716	1126069.623141	43.312461
3508.534327	1125897.389822	43.317466
3508.256811	1125739.603040	43.322471
3508.635633	1125576.185290	43.327476
3508.617293	1125411.686215	43.332481
3508.289294	1125240.763041	43.337485
3508.459413	1125071.369911	43.342490
3508.439010	1124904.762232	43.347495
3508.341135	1124732.547878	43.352500
3508.761914	1124572.613278	43.357505
3508.478270	1124403.178510	43.362509
3508.426222	1124229.893600	43.367514
3507.969183	1124081.128029	43.372519
3508.074926	1123919.322378	43.377524
3508.404062	1123750.717682	43.382529
3508.122576	1123585.539424	43.387533
3508.256281	1123412.768456	43.392538
3508.190043	1123264.582018	43.397543
3508.205718	1123099.244589	43.402548
3508.500211	1122937.663665	43.407553
3508.032360	1122789.910951	43.412557
3508.385125	1122615.269475	43.417562
3508.178461	1122465.275293	43.422567
3508.555294	1122287.858442	43.427572
3508.317581	1122124.722181	43.432577
3508.408378	1121964.954244	43.437581
3508.405733	1121809.386102	43.442586
3507.934671	1121638.371096	43.447591
3507.985322	1121473.358429	43.452596
3508.026162	1121316.340551	43.457601
3508.182155	1121166.059725	43.462605
3508.250963	1121017.693490	43.467610
3507.962373	1120850.527343	43.472615
3507.977700	1120689.971916	43.477620
3507.760145	1120525.735996	43.482625
3507.504469	1120369.215289	43.487629
3507.862090	1120227.445953	43.492634
3507.882566	1120082.966447	43.497639
3507.741400	1119918.127844	43.502644
3508.084572	1119768.157875	43.507649
3508.043000	1119613.675180	43.512653
3508.092795	1119451.267180	43.517658
3507.716953	1119293.972783	43.522663
3507.715594	1119148.233330	43.527668
3507.874440	1119004.749729	43.532673
3507.578856	1118842.951695	43.537677
3507.759350	1118687.929387	43.542682
3507.376335	1118548.047556	43.547687
3507.540061	1118387.684376	43.552692
3507.311318	1118241.386055	43.557697
3507.267739	1118091.909171	43.562701
3507.482017	1117946.863685	43.567706
3507.430203	1117807.574890	43.572711
3507.457131	1117656.263912	43.577716
3507.000032	1117510.554918	43.582721
3506.855579	1117373.271067	43.587725
3506.999739	1117230.123467	43.592730
3507.067960	1117101.945482	43.597735
3507.400029	1116955.710245	43.602740
3507.305653	1116827.266581	43.607745
3507.056958	1116678.165198	43.612749
3507.349429	1116536.975952	43.617754
3507.436916	1116400.867908	43.622759
3507.071753	1116255.204908	43.627764
3507.124714	1116125.290533	43.632769
3507.298172	1115974.384457	43.637773
3507.367518	1115827.494516	43.642778
3507.223325	1115686.545413	43.647783
3507.166863	1115544.815592	43.652788
3507.350974	1115410.477564	43.657793
3507.316787	1115263.779870	43.662797
3507.562713	1115127.041432	43.667802
3507.391969	1114989.033511	43.672807
3507.186695	1114833.677186	43.677812
3507.053271	1114693.748860	43.682817
3506.953872	1114553.620602	43.687821
3507.318787	1114415.509697	43.692826
3506.997797	1114272.264352	43.697831
3507.188014	1114125.403210	43.702836
3507.224468	1114000.874752	43.707841
3507.077942	1113859.210549	43.712845
3506.806329	1113705.262702	43.717850
3506.774097	1113578.828701	43.722855
3506.770021	1113445.712065	43.727860
3507.089869	1113316.353170	43.732865
3506.933589	1113180.966399	43.737869
3506.966772	1113048.310580	43.742874
3506.446283	1112905.443037	43.747879
3506.576084	1112769.331193	43.752884
3506.710991	1112650.668084	43.757889
3506.636845	1112518.398329	43.762893
3506.837494	1112377.973067	43.767898
3506.555085	1112256.413304	43.772903
3506.329295	1112117.100613	43.777908
3506.738555	1112003.051678	43.782913
3506.185065	1111873.229544	43.787917
3506.634132	1111734.845029	43.792922
3506.480499	1111620.308346	43.797927
3506.603431	1111487.408390	43.802932
3506.362299	1111363.818375	43.807937
3506.296910	1111233.328008	43.812941
3506.407893	1111108.720162	43.817946
3506.232005	1110998.466830	43.822951
3506.393376	1110863.255479	43.827956
3506.617774	1110736.235233	43.832961
3506.415057	1110607.755802	43.837965
3506.696670	1110492.169296	43.842970
3506.240774	1110370.499987	43.847975
3506.587764	1110230.757783	43.852980
3506.702622	1110101.259791	43.857985
3506.482372	1109992.806044	43.862989
3506.759975	1109857.454827	43.867994
3506.586374	1109732.289405	43.872999
3506.364325	1109602.357763	43.878004
3506.574726	1109476.264303	43.883009
3506.295468	1109353.206867	43.888013
3506.399878	1109224.166617	43.893018
3506.304818	1109105.272193	43.898023
3506.521547	1108988.232522	43.903028
3506.471689	1108852.528194	43.908033
3505.868758	1108740.390070	43.913037
3506.415004	1108616.988940	43.918042
3506.031444	1108503.473538	43.923047
3506.005312	1108378.920428	43.928052
3506.215371	1108254.325534	43.933057
3505.877618	1108129.627074	43.938061
3506.391820	1108008.985385	43.943066
3506.285521	1107898.943352	43.948071
3506.308889	1107781.813823	43.953076
3506.094149	1107656.511384	43.958081
3506.038530	1107541.967068	43.963085
3506.031186	1107418.056851	43.968090
3505.579568	1107302.999878	43.973095
3505.831318	1107179.996173	43.978100
3505.749949	1107070.124016	43.983105
3506.250114	1106966.168612	43.988109
3506.278172	1106852.073192	43.993114
3505.985465	1106743.183912	43.998119
3506.077317	1106606.349334	44.003124
3506.059239	1106496.741486	44.008129
3505.945140	1106379.222144	44.013133
3505.757350	1106264.767892	44.018138
3505.436970	1106161.505006	44.023143
3505.712359	1106051.744278	44.028148
3505.756772	1105942.305827	44.033153
3505.980507	1105825.769162	44.038157
3506.409660	1105706.426796	44.043162
3505.582019	1105604.096213	44.048167
3505.852499	1105488.690517	44.053172
3506.023502	1105369.956206	44.058177
3505.614537	1105255.039409	44.063181
3506.043040	1105147.145093	44.068186
3506.102608	1105044.180217	44.073191
3506.163044	1104925.836356	44.078196
3506.146898	1104803.491055	44.083201
3505.781308	1104688.268486	44.088205
3506.093057	1104558.413607	44.093210
3506.300721	1104460.666524	44.098215
3506.051008	1104334.719402	44.103220
3505.979104	1104206.256493	44.108225
3505.861588	1104094.896750	44.113229
3505.837663	1103984.665597	44.118234
3505.662595	1103886.589036	44.123239
3505.628896	1103774.158062	44.128244
3505.956923	1103662.811542	44.133249
3505.586367	1103548.902852	44.138253
3506.075651	1103425.774299	44.143258
3505.763614	1103330.480698	44.148263
3505.886364	1103225.655470	44.153268
3505.543858	1103106.860335	44.158273
3505.585233	1102999.082335	44.163277
3505.794862	1102888.217039	44.168282
3505.515613	1102790.997602	44.173287
3505.565608	1102676.045735	44.178292
3505.876155	1102571.559060	44.183297
3505.477222	1102461.071863	44.188301
3505.329304	1102346.718885	44.193306
3505.131600	1102239.442852	44.198311
3505.242479	1102143.771947	44.203316
3505.373144	1102053.447427	44.208321
3505.398498	1101949.664597	44.213325
3505.646186	1101835.426749	44.218330
3505.595739	1101731.365515	44.223335
3505.314778	1101634.125499	44.228340
3505.387248	1101529.275587	44.233345
3505.481107	1101419.163723	44.238349
3505.710153	1101321.069503	44.243354
3505.501772	1101217.215509	44.248359
3505.428494	1101105.882314	44.253364
3505.644519	1101000.042715	44.258369
3505.295360	1100899.837769	44.263373
3505.312016	1100792.879983	44.268378
3505.276553	1100694.244446	44.273383
3505.585313	1100591.153485	44.278388
3505.364524	1100490.728628	44.283393
3505.009071	1100386.978463	44.288397
3505.064860	1100282.871800	44.293402
3505.279004	1100192.311207	44.298407
3505.032898	1100091.978691	44.303412
3505.472490	1099997.362738	44.308417
3505.151104	1099884.515678	44.313421
3505.509634	1099782.548265	44.318426
3505.309518	1099694.628749	44.323431
3505.209302	1099602.198009	44.328436
3505.235385	1099488.807436	44.333441
3505.452516	1099390.775722	44.338445
3505.508833	1099285.215643	44.343450
3505.283401	1099184.958476	44.348455
3505.198738	1099096.436543	44.353460
3505.172294	1098983.808917	44.358465
3504.922837	1098885.940502	44.363469
3505.228372	1098793.620332	44.368474
3505.053795	1098700.038993	44.373479
3505.133921	1098601.250570	44.378484
3505.190071	1098499.213126	44.383489
3505.258698	1098392.007987	44.388493
3505.547576	1098296.143963	44.393498
3505.176664	1098209.280281	44.398503
3505.198090	1098095.096206	44.403508
3505.429710	1098008.799475	44.408513
3504.744566	1097913.662872	44.413517
3505.054841	1097800.094423	44.418522
3505.034180	1097710.104713	44.423527
3504.911992	1097614.009387	44.428532
3504.837015	1097526.512157	44.433537
3504.966717	1097433.719530	44.438541
3505.202837	1097333.734557	44.443546
3504.873320	1097239.101359	44.448551
3504.906676	1097136.276785	44.453556
3505.121050	1097040.785366	44.458561
3505.071974	1096950.022499	44.463565
3505.048450	1096856.193051	44.468570
3504.861929	1096760.762715	44.473575
3504.700015	1096667.622360	44.478580
3504.815621	1096575.582572	44.483585
3504.673734	1096481.861780	44.488589
3504.861009	1096388.180811	44.493594
3504.952623	1096308.289213	44.498599
3504.286296	1096222.590177	44.503604
3504.467418	1096140.194122	44.508609
3504.201105	1096051.843563	44.513613
3504.402026	1095965.614957	44.518618
3504.609895	1095886.845998	44.523623
3504.513499	1095805.638580	44.528628
3504.607632	1095714.735728	44.533633
3504.848177	1095639.114949	44.538637
3505.064139	1095549.720031	44.543642
3504.622083	1095466.650961	44.548647
3504.868282	1095362.513828	44.553652
3505.044086	1095271.494404	44.558657
3504.768149	1095169.927229	44.563661
3504.667425	1095083.829940	44.568666
3504.823167	1094996.062407	44.573671
3504.590087	1094907.400629	44.578676
3504.490995	1094807.711248	44.583681
3504.272836	1094725.550797	44.588685
3504.620762	1094646.836420	44.593690
3504.318160	1094572.916947	44.598695
3504.319729	1094485.549298	44.603700
3504.672000	1094399.270821	44.608705
3504.150257	1094322.800256	44.613709
3504.479508	1094237.384259	44.618714
3504.442167	1094163.511203	44.623719
3504.552488	1094077.841651	44.628724
3504.742017	1093977.802353	44.633729
3504.488616	1093903.578526	44.638733
3504.620721	1093807.469391	44.643738
3504.560680	1093737.901013	44.648743
3504.409481	1093636.380218	44.653748
3504.487615	1093558.268715	44.658753
3504.380161	1093485.642188	44.663757
3504.488172	1093398.239469	44.668762
3504.293376	1093317.968059	44.673767
3504.290653	1093241.683875	44.678772
3504.332459	1093159.743990	44.683777
3504.124508	1093082.725633	44.688781
3504.333045	1092998.362891	44.693786
3504.238844	1092926.588163	44.698791
3503.982969	1092849.574383	44.703796
3504.063902	1092766.569162	44.708801
3504.092134	1092683.284174	44.713805
3504.299764	1092603.893156	44.718810
3504.508053	1092543.455001	44.723815
3504.216667	1092459.740579	44.728820
3504.262563	1092375.203468	44.733825
3504.314287	1092298.514116	44.738829
3504.726424	1092226.838193	44.743834
3504.383888	1092146.382287	44.748839
3504.435299	1092062.318062	44.753844
3504.416318	1091977.306750	44.758849
3504.400550	1091895.931667	44.763853
3504.232488	1091803.283036	44.768858
3504.465827	1091723.204705	44.773863
3503.945898	1091660.674574	44.778868
3504.145404	1091574.950764	44.783873
3504.020065	1091503.258057	44.788877
3504.152939	1091420.702406	44.793882
3504.233863	1091350.792916	44.798887
3504.170290	1091277.746570	44.803892
3503.971894	1091196.391065	44.808897
3504.154475	1091114.397076	44.813901
3504.157690	1091042.198334	44.818906
3504.269825	1090974.385447	44.823911
3504.134360	1090886.312037	44.828916
3504.165937	1090811.041321	44.833921
3504.057898	1090737.995028	44.838925
3504.112018	1090658.983862	44.843930
3504.154180	1090585.336209	44.848935
3503.601550	1090501.059976	44.853940
3503.800390	1090444.143249	44.858945
3503.801169	1090387.737373	44.863949
3503.813359	1090308.153408	44.868954
3504.185123	1090243.353176	44.873959
3503.951354	1090164.573761	44.878964
3503.945339	1090085.755690	44.883969
3503.958285	1090024.651248	44.888973
3503.825204	1089957.823764	44.893978
3503.640312	1089891.003990	44.898983
3503.849095	1089810.518377	44.903988
3504.227881	1089744.561725	44.908993
3503.930861	1089677.566236	44.913997
3504.208018	1089593.235005	44.919002
3504.271839	1089523.400566	44.924007
3504.235112	1089444.674025	44.929012
3504.218353	1089376.575052	44.934017
3503.701143	1089301.756916	44.939021
3503.881827	1089216.094727	44.944026
3503.969398	1089146.251524	44.949031
3503.839739	1089074.240053	44.954036
3504.290213	1089007.592125	44.959041
3503.872658	1088943.672707	44.964045
3503.961369	1088862.618072	44.969050
3503.829843	1088780.353174	44.974055
3503.929261	1088718.070250	44.979060
3504.351512	1088648.069725	44.984065
3504.049863	1088579.911882	44.989069
3503.977465	1088506.829678	44.994074
3504.254163	1088445.759822	44.999079
3503.966408	1088372.902883	45.004084
3504.087310	1088294.421103	45.009089
3504.093470	1088217.106737	45.014093
3503.897502	1088138.291672	45.019098
3504.129559	1088065.057574	45.024103
3504.462245	1087997.650209	45.029108
3504.051505	1087919.154759	45.034113
3504.010331	1087838.010415	45.039117
3504.282976	1087764.765586	45.044122
3504.301794	1087694.435976	45.049127
3503.911756	1087625.130939	45.054132
3503.790768	1087551.756440	45.059137
3503.695306	1087478.951647	45.064141
3503.940576	1087410.880682	45.069146
3503.886847	1087349.086377	45.074151
3503.812677	1087273.784022	45.079156
3504.100883	1087195.929567	45.084161
3503.650441	1087141.289069	45.089165
3503.997037	1087068.501795	45.094170
3503.973342	1086986.383607	45.099175
3503.914246	1086909.827990	45.104180
3503.726737	1086851.883149	45.109185
3503.448734	1086787.148713	45.114189
3503.956952	1086726.213067	45.119194
3503.729604	1086645.560726	45.124199
3503.333515	1086584.772431	45.129204
3503.757493	1086519.344193	45.134209
3503.579666	1086467.335365	45.139213
3503.942315	1086388.211229	45.144218
3503.858777	1086326.122690	45.149223
3503.611251	1086264.922997	45.154228
3503.660177	1086183.643267	45.159233
3503.359592	1086125.325939	45.164237
3503.547114	1086055.139009	45.169242
3503.588757	1085996.668094	45.174247
3503.198912	1085931.654352	45.179252
3503.200911	1085857.374112	45.184257
3503.206632	1085809.833509	45.189261
3503.550653	1085755.335754	45.194266
3503.423791	1085687.592047	45.199271
3503.843912	1085626.371052	45.204276
3503.824183	1085566.372021	45.209281
3503.897991	1085511.820481	45.214285
3503.858613	1085433.515488	45.219290
3503.698137	1085369.607483	45.224295
3503.304565	1085299.123085	45.229300
3503.740086	1085241.058454	45.234305
3503.486387	1085180.710275	45.239309
3503.506266	1085114.660700	45.244314
3503.555126	1085038.060939	45.249319
3503.436329	1084984.590294	45.254324
3503.571692	1084924.750364	45.259329
3503.573857	1084863.302037	45.264333
3503.428594	1084797.275806	45.269338
3503.377688	1084739.381803	45.274343
3503.509007	1084670.624249	45.279348
3503.543112	1084615.399192	45.284353
3503.528142	1084557.017992	45.289357
3503.506735	1084498.253746	45.294362
3503.426572	1084434.321520	45.299367
3503.154964	1084368.406761	45.304372
3503.583143	1084307.073734	45.309377
3503.147252	1084268.987947	45.314381
3503.686118	1084192.679077	45.319386
3503.596426	1084130.758230	45.324391
3503.677466	1084062.960042	45.329396
3503.778850	1084001.293884	45.334401
3503.477010	1083947.172037	45.339405
3503.450677	1083869.705297	45.344410
3503.768692	1083816.342987	45.349415
3503.215375	1083757.658346	45.354420
3503.477450	1083696.825219	45.359425
3503.013411	1083647.425406	45.364429
3503.742798	1083577.117270	45.369434
3503.631170	1083534.370401	45.374439
3503.496793	1083470.819329	45.379444
3503.802424	1083396.647255	45.384449
3503.488170	1083330.918724	45.389453
3503.454849	1083260.444448	45.394458
3503.198944	1083218.485991	45.399463
3503.280398	1083163.142507	45.404468
3503.531807	1083087.728544	45.409473
3503.467804	1083015.338257	45.414477
3503.563528	1082951.455536	45.419482
3503.551981	1082902.933404	45.424487
3503.450155	1082838.794203	45.429492
3503.539505	1082774.430961	45.434497
3503.720747	1082725.204193	45.439501
3503.590592	1082654.929829	45.444506
3503.830192	1082590.539669	45.449511
3503.625254	1082531.208991	45.454516
3503.518673	1082469.367925	45.459521
3503.505138	1082421.896794	45.464525
3503.600117	1082338.537997	45.469530
3503.436080	1082284.280999	45.474535
3502.808516	1082218.398810	45.479540
3503.352802	1082159.707967	45.484545
3502.929464	1082111.438423	45.489549
3503.019625	1082050.423402	45.494554
3503.249861	1081994.659889	45.499559
3503.007828	1081944.440727	45.504564
3503.706183	1081884.186910	45.509569
3503.259439	1081826.902610	45.514573
3503.042219	1081762.961574	45.519578
3502.860146	1081717.718172	45.524583
3503.171949	1081663.952135	45.529588
3503.074360	1081612.363245	45.534593
3503.044974	1081566.997524	45.539597
3503.124852	1081505.210721	45.544602
3503.081305	1081458.407591	45.549607
3503.060320	1081403.254944	45.554612
3503.069592	1081338.887929	45.559617
3502.998208	1081311.369082	45.564621
3503.171319	1081249.276244	45.569626
3503.319931	1081184.404822	45.574631
3503.059643	1081134.373050	45.579636
3503.186669	1081076.698567	45.584641
3502.904830	1081039.044420	45.589645
3502.858850	1080972.379840	45.594650
3503.332340	1080915.318111	45.599655
3503.224146	1080867.369358	45.604660
3503.063557	1080803.311794	45.609665
3502.766393	1080758.463117	45.614669
3502.948471	1080695.211265	45.619674
3503.123989	1080649.420411	45.624679
3503.109926	1080606.346667	45.629684
3503.039973	1080553.112245	45.634689
3502.896143	1080515.335806	45.639693
3502.840124	1080464.208896	45.644698
3503.180660	1080411.385187	45.649703
3503.197958	1080357.750720	45.654708
3503.316748	1080300.453153	45.659713
3503.112530	1080250.499970	45.664717
3502.915777	1080191.526226	45.669722
3503.191269	1080144.371429	45.674727
3503.064594	1080090.086416	45.679732
3503.323994	1080031.995292	45.684737
3503.078056	1079985.404741	45.689741
3503.071871	1079927.452194	45.694746
3503.353672	1079877.607448	45.699751
3503.308826	1079815.438229	45.704756
3503.392142	1079758.908433	45.709761
3503.067290	1079706.955118	45.714765
3503.021923	1079658.985385	45.719770
3503.268703	1079608.568220	45.724775
3502.738889	1079564.323760	45.729780
3503.172453	1079508.885167	45.734785
3503.025222	1079454.021459	45.739789
3502.962075	1079403.557485	45.744794
3502.662329	1079349.869360	45.749799
3502.495315	1079310.265138	45.754804
3502.971098	1079269.019373	45.759809
3502.671013	1079217.153270	45.764813
3502.687131	1079143.066958	45.769818
3502.937300	1079032.570125	45.774823
3502.709715	1078874.453497	45.779828
3502.760696	1078640.276449	45.784833
3502.547950	1078351.425648	45.789837
3502.691372	1077997.136081	45.794842
3502.722967	1077589.567017	45.799847
3502.133995	1077111.702387	45.804852
3502.441176	1076562.601852	45.809857
3502.042667	1075967.857095	45.814861
3502.471720	1075308.666641	45.819866
3502.552117	1074566.184198	45.824871
3501.849668	1073761.868458	45.829876
3501.891802	1072881.798075	45.834881
3501.670419	1071937.921805	45.839885
3501.831222	1070915.011334	45.844890
3501.703963	1069830.820412	45.849895
3501.416216	1068673.561724	45.854900
3501.345592	1067428.028322	45.859905
3501.119363	1066107.592508	45.864909
3501.258667	1064698.355521	45.869914
3500.788834	1063223.797067	45.874919
3500.569446	1061671.304373	45.879924
3500.216100	1060045.786443	45.884929
3499.738481	1058321.457602	45.889933
3499.774130	1056516.332783	45.894938
3499.448120	1054639.827626	45.899943
3498.988220	1052689.228919	45.904948
3498.922720	1050634.854213	45.909953
3498.575386	1048526.494517	45.914957
3498.283608	1046331.693277	45.919962
3497.884381	1044039.752147	45.924967
3497.518958	1041672.751247	45.929972
3497.166565	1039207.883837	45.934977
3496.546939	1036674.466344	45.939981
3496.417483	1034062.510216	45.944986
3496.113494	1031369.402985	45.949991
3495.609443	1028582.830735	45.954996
3495.279486	1025706.470136	45.960001
3494.512579	1022770.242828	45.965005
3494.245195	1019738.013224	45.970010
3493.753561	1016639.834674	45.975015
3493.078355	1013440.247077	45.980020
3492.778412	1010159.296438	45.985025
3492.027690	1006807.772401	45.990029
3491.420275	1003377.478218	45.995034
3491.234031	999854.114438	46.000039
3490.518389	996246.922149	46.005044
3490.022886	992553.088648	46.010049
3489.434077	988802.249520	46.015053
3488.658020	984948.442112	46.020058
3488.310153	981005.621474	46.025063
3487.648001	977003.248059	46.030068
3487.295430	972900.316661	46.035073
3486.081513	968723.335945	46.040077
3485.543480	964445.550537	46.045082
3485.154004	960097.708068	46.050087
3484.217012	955670.454220	46.055092
3483.896210	951242.919494	46.060097
3482.994489	946762.755388	46.065101
3481.982561	942190.151728	46.070106
3481.123526	937548.460000	46.075111
3480.162836	932827.207832	46.080116
3479.306604	928010.235278	46.085121
3478.374031	923126.023823	46.090125
3477.587068	918157.934546	46.095130
3476.728940	913109.868533	46.100135
3475.275390	907995.728312	46.105140
3474.410539	902775.117216	46.110145
3473.218711	897489.596362	46.115149
3472.580533	892133.670804	46.120154
3471.992244	886694.115256	46.125159
3470.704283	881163.220468	46.130164
3469.813036	875547.399345	46.135169
3468.559532	869854.853660	46.140173
3467.780203	864075.671122	46.145178
3466.746242	858221.078879	46.150183
3465.585596	852270.753258	46.155188
3464.455035	846243.670270	46.160193
3463.347242	840152.225017	46.165197
3461.897317	833948.467870	46.170202
3460.967062	827669.456259	46.175207
3459.799181	821323.354013	46.180212
3458.676057	814882.535020	46.185217
3457.248967	808367.708048	46.190221
3455.912087	801767.403062	46.195226
3454.933700	795084.766416	46.200231
3453.475330	788329.287707	46.205236
3452.403332	781483.199772	46.210241
3450.788175	774542.463752	46.215245
3449.345115	767550.629796	46.220250
3447.633119	760464.212518	46.225255
3446.275597	753310.024576	46.230260
3445.225180	746063.775642	46.235265
3443.731468	738751.680386	46.240269
3442.211538	731341.465269	46.245274
3441.153172	723840.937791	46.250279
3439.018514	716279.213332	46.255284
3437.967382	708620.391981	46.260289
3436.592037	700894.705485	46.265293
3434.481667	693087.605032	46.270298
3433.025333	685201.229456	46.275303
3431.473883	677244.463093	46.280308
3429.815065	669198.020734	46.285313
3428.246326	661078.468228	46.290317
3426.702736	652895.381346	46.295322
3425.132899	644615.964950	46.300327
3422.870309	636277.940551	46.305332
3421.565991	627846.399625	46.310337
3419.835188	619356.004228	46.315341
3417.690871	610777.390007	46.320346
3416.005981	602138.951372	46.325351
3413.796679	593428.937298	46.330356
3411.894817	584647.183826	46.335361
3410.080750	575782.134742	46.340365
3408.101820	566852.069689	46.345370
3406.323251	557851.242317	46.350375
3404.059288	548786.825636	46.355380
3402.288961	539642.285201	46.360385
3400.259268	530433.391727	46.365389
3397.963167	521159.777124	46.370394
3395.867376	511805.383764	46.375399
3393.444608	502399.801049	46.380404
3391.596167	492932.029355	46.385409
3389.369013	483396.874875	46.390413
3387.095506	473787.661481	46.395418
3384.850016	464104.591420	46.400423
3382.154330	454381.379464	46.405428
3380.114179	444580.788452	46.410433
3377.208349	434733.295313	46.415437
3374.614645	424826.118273	46.420442
3372.426981	414849.966706	46.425447
3369.711035	404829.550387	46.430452
3367.209299	394747.085406	46.435457
3364.095917	384625.167692	46.440461
3361.938604	374441.484312	46.445466
3358.945483	364206.559017	46.450471
3356.091727	353939.535338	46.455476
3353.635501	343615.345662	46.460481
3350.381152	333243.048190	46.465485
3347.164038	322836.624833	46.470490
3344.208795	312369.946830	46.475495
3341.070803	301884.286685	46.480500
3337.995902	291356.604230	46.485505
3334.831073	280802.656988	46.490509
3331.563480	270186.513894	46.495514
3328.316338	259558.765153	46.500519
3324.820660	248901.869595	46.505524
3321.365912	238210.524956	46.510529
3317.755863	227421.837498	46.515533
3314.049567	216670.057622	46.520538
3310.108834	205917.630800	46.525543
3305.982150	195148.651730	46.530548
3302.163441	184372.515305	46.535553
3298.199331	173599.187581	46.540557
3293.657785	162816.224604	46.545562
3289.267900	152023.059549	46.550567
3284.429711	141248.369151	46.555572
3280.079400	130497.782268	46.560577
3274.770109	119751.750989	46.565581
3269.064047	109022.271346	46.570586
3263.229064	98329.187265	46.575591
3257.099847	87703.561592	46.580596
3251.023582	77102.724562	46.585601
3243.862846	66589.949983	46.590605
3235.745825	56166.820803	46.595610
3224.593034	45912.637729	46.600615
3199.186768	36189.419303	46.605620
3170.627453	26813.436322	46.610625
3141.563732	17866.862148	46.615629
3111.473033	9463.837282	46.620634
3064.277137	2138.485140	46.625639
2842.456991	436.491361	46.630644
2643.715657	413.865565	46.635649
2568.242423	388.456266	46.640653
2594.838349	382.790333	46.645658
2676.750881	377.062446	46.650663
2765.422933	370.667325	46.655668
2832.438339	372.152242	46.660673
2868.132583	357.541450	46.665677
2875.886912	354.425063	46.670682
2868.516311	349.405748	46.675687
2854.066427	362.227549	46.680692
2840.842181	368.845341	46.685697
2831.868780	357.380434	46.690701
2827.077753	367.673880	46.695706
2825.348747	343.674802	46.700711
2824.207975	331.761490	46.705716
2823.521283	350.227541	46.710721
2821.920327	349.851320	46.715725
2819.813684	341.794651	46.720730
2816.965661	330.193186	46.725735
2813.755076	342.881261	46.730740
2810.934458	330.809119	46.735745
2808.000572	333.249136	46.740749
2804.464080	349.131829	46.745754
2801.325162	332.292118	46.750759
2798.262536	336.156578	46.755764
2795.640700	326.528589	46.760769
2792.426590	323.338118	46.765773
2788.996545	327.247368	46.770778
2785.460990	318.210240	46.775783
2782.209907	334.770811	46.780788
2779.334819	322.812644	46.785793
2776.309322	325.173062	46.790797
2773.030404	334.952226	46.795802
2769.895325	315.997576	46.800807
2766.316930	320.619431	46.805812
2763.032907	325.405956	46.810817
2759.462519	326.204973	46.815821
2756.453241	310.469925	46.820826
2753.201499	308.317445	46.825831
2749.313996	319.799445	46.830836
2746.155701	310.801862	46.835841
2742.818235	305.864002	46.840845
2739.555487	306.939951	46.845850
2736.573930	312.167142	46.850855
2732.726968	313.695174	46.855860
2729.470882	311.753266	46.860865
2726.220457	304.888776	46.865869
2722.944642	307.365066	46.870874
2719.944591	304.488590	46.875879
2716.122326	316.327739	46.880884
2712.575573	297.893564	46.885889
2709.077859	307.335879	46.890893
2705.759495	308.836263	46.895898
2702.624004	295.911227	46.900903
2698.827413	300.854397	46.905908
2695.362309	301.835472	46.910913
2692.280787	296.157338	46.915917
2688.232942	298.340647	46.920922
2685.620065	294.620165	46.925927
2681.667568	296.798905	46.930932
2678.063962	292.460799	46.935937
2674.966132	291.795799	46.940941
2671.391765	292.833573	46.945946
2668.600241	292.427462	46.950951
2665.385709	301.052877	46.955956
2661.652518	291.040334	46.960961
2658.262905	289.631721	46.965965
2654.434655	292.932248	46.970970
2651.035150	291.456110	46.975975
2647.028531	298.199905	46.980980
2643.428230	291.140093	46.985985
2640.188919	291.066505	46.990989
2636.892245	290.551906	46.995994
2634.221172	287.822488	47.000999
2629.945161	292.698720	47.006004
2626.871068	292.613090	47.011009
2623.468697	278.053751	47.016013
2619.729175	280.985185	47.021018
2616.174036	288.680686	47.026023
2612.520518	297.929600	47.031028
2609.289413	286.703588	47.036033
2605.510659	281.132571	47.041037
2602.657302	286.421729	47.046042
2599.565124	269.719329	47.051047
2596.626484	285.718711	47.056052
2592.637093	279.684409	47.061057
2588.909346	280.772570	47.066061
2585.264689	269.763944	47.071066
2581.839486	265.789531	47.076071
2578.163904	275.489889	47.081076
2574.750555	278.235458	47.086081
2571.768062	275.551299	47.091085
2567.514077	274.229021	47.096090
2564.409439	263.489594	47.101095
2560.827721	276.530415	47.106100
2557.641973	271.692737	47.111105
2554.225914	261.021736	47.116109
2550.581512	272.037787	47.121114
2547.459632	269.194304	47.126119
2543.405506	278.247256	47.131124
2539.903836	278.342663	47.136129
2536.268802	267.067882	47.141133
2532.874084	266.962054	47.146138
2529.732930	270.252827	47.151143
2526.090884	270.464717	47.156148
2522.649494	273.824141	47.161153
2519.553823	268.604918	47.166157
2515.711684	276.252770	47.171162
2512.664619	255.030306	47.176167
2508.727313	272.529008	47.181172
2505.205095	272.708422	47.186177
2501.675781	265.905934	47.191181
2498.108392	269.477836	47.196186
2495.110104	264.747891	47.201191
2491.671099	274.339420	47.206196
2487.769512	268.767319	47.211201
2484.608854	267.077941	47.216205
2480.924265	261.659486	47.221210
2477.573792	249.502595	47.226215
2473.524442	253.899337	47.231220
2470.592039	254.555493	47.236225
2467.109902	263.881251	47.241229
2463.269751	260.722752	47.246234
2460.051328	254.308543	47.251239
2456.490309	259.868144	47.256244
2452.708478	254.567853	47.261249
2449.393079	250.799058	47.266253
2445.949883	262.889783	47.271258
2442.810832	244.023884	47.276263
2439.279335	256.065435	47.281268
2435.606302	260.888887	47.286273
2432.606990	253.941622	47.291277
2428.677143	249.360993	47.296282
2425.494255	249.305916	47.301287
2421.215686	248.553085	47.306292
2417.640694	251.435276	47.311297
2414.802816	244.587386	47.316301
2411.135767	249.083600	47.321306
2407.627468	251.985183	47.326311
2404.293480	249.305889	47.331316
2401.084556	244.035459	47.336321
2397.513890	250.741885	47.341325
2393.567953	250.987676	47.346330
2390.309399	241.804503	47.351335
2386.451918	241.750197	47.356340
2382.989086	249.196334	47.361345
2379.858610	250.193493	47.366349
2375.876805	247.672744	47.371354
2373.243754	235.826472	47.376359
2369.238037	249.256119	47.381364
2365.553315	252.627813	47.386369
2362.234023	243.791882	47.391373
2358.500818	243.077204	47.396378
2355.441276	248.091635	47.401383
2352.126072	247.908648	47.406388
2348.841995	238.393387	47.411393
2345.224398	249.591538	47.416397
2340.924512	254.656037	47.421402
2337.401011	229.116722	47.426407
2334.432616	244.016066	47.431412
2330.889567	247.794358	47.436417
2327.584496	241.334132	47.441421
2323.917340	246.531655	47.446426
2320.366227	243.068962	47.451431
2317.081387	250.933969	47.456436
2313.295180	239.571608	47.461441
2309.527537	237.202434	47.466445
2306.253058	249.654867	47.471450
2303.247160	238.882242	47.476455
2299.317683	250.534565	47.481460
2295.749143	251.589997	47.486465
2292.573423	238.159841	47.491469
2288.945353	246.052458	47.496474
2285.460662	244.312923	47.501479
2281.826047	245.005645	47.506484
2278.401422	249.769152	47.511489
2274.927434	246.519093	47.516493
2271.169173	257.328780	47.521498
2268.053157	236.801463	47.526503
2264.256432	234.778857	47.531508
2261.075438	238.565635	47.536513
2257.915240	243.628271	47.541517
2253.672659	246.805721	47.546522
2250.465841	236.810630	47.551527
2246.607749	250.679862	47.556532
2243.274091	246.395538	47.561537
2240.143402	245.486242	47.566541
2236.327923	236.552664	47.571546
2232.946603	231.915423	47.576551
2229.716705	240.674302	47.581556
2225.922084	241.089380	47.586561
2222.577654	231.425505	47.591565
2218.630092	245.918213	47.596570
2215.595106	237.887276	47.601575
2211.825662	233.283477	47.606580
2208.524253	244.360167	47.611585
2205.427748	240.848596	47.616589
2201.554264	230.158158	47.621594
2198.212937	224.139853	47.626599
2194.519932	234.777882	47.631604
2190.725962	239.332613	47.636609
2187.412301	236.518463	47.641613
2184.108043	238.482000	47.646618
2180.629913	229.670400	47.651623
2177.136031	233.901472	47.656628
2173.200752	229.127341	47.661633
2169.939013	237.117823	47.666637
2166.439476	240.185288	47.671642
2163.099457	224.317869	47.676647
2159.308909	233.551341	47.681652
2156.142190	224.553924	47.686657
2152.591550	225.428690	47.691661
2149.174203	229.047611	47.696666
2145.499428	216.115220	47.701671
2142.056587	230.891004	47.706676
2138.300640	228.913535	47.711681
2134.691573	228.546584	47.716685
2131.321635	232.380756	47.721690
2127.942070	236.696583	47.726695
2124.472995	236.298060	47.731700
2120.680988	229.351581	47.736705
2118.033745	224.221773	47.741709
2113.966000	225.524981	47.746714
2110.278050	229.764809	47.751719
2107.072374	231.878255	47.756724
2103.376347	228.585001	47.761729
2100.315701	223.083482	47.766733
2096.611601	228.463097	47.771738
2092.926685	234.813886	47.776743
2089.245159	234.842289	47.781748
2086.204310	223.353977	47.786753
2082.833559	222.547688	47.791757
2078.971766	226.950181	47.796762
2075.575014	212.120092	47.801767
2072.683869	228.964484	47.806772
2068.696937	220.758086	47.811777
2064.783639	218.409718	47.816781
2061.358504	227.247024	47.821786
2058.041807	212.822340	47.826791
2054.867539	221.834815	47.831796
2051.190963	220.273457	47.836801
2047.527083	218.024146	47.841805
2044.067530	223.414645	47.846810
2040.343916	213.927086	47.851815
2036.829461	213.928746	47.856820
2033.296052	220.797765	47.861825
2029.988522	215.074089	47.866829
2026.236468	221.819060	47.871834
2023.154122	218.173141	47.876839
2019.886747	209.404915	47.881844
2016.069176	220.653124	47.886849
2012.724073	216.500841	47.891853
2009.111994	218.360241	47.896858
2005.429691	214.802352	47.901863
2001.806434	218.090765	47.906868
1998.597901	218.145862	47.911873
1995.286982	219.705394	47.916877
1991.524482	216.097010	47.921882
1988.072227	214.474016	47.926887
1984.531522	216.825788	47.931892
1980.836139	220.571051	47.936897
1977.248291	216.198575	47.941901
1973.725198	216.991929	47.946906
1970.465109	219.882152	47.951911
1967.281838	228.067035	47.956916
1963.450142	220.526480	47.961921
1960.406288	215.704568	47.966925
1956.526873	229.766532	47.971930
1953.344657	219.418607	47.976935
1949.340515	226.302378	47.981940
1945.975786	225.102111	47.986945
1942.696682	219.237445	47.991949
1938.919335	228.144939	47.996954
1935.599463	221.327861	48.001959
1931.859750	215.898103	48.006964
1928.388169	221.666220	48.011969
1925.160474	225.689713	48.016973
1921.496784	233.183364	48.021978
1918.117510	220.487285	48.026983
1914.377065	218.378238	48.031988
1911.048990	216.923228	48.036993
1907.141212	216.499418	48.041997
1904.086295	218.027213	48.047002
1900.687176	218.431370	48.052007
1897.242227	220.543829	48.057012
1893.453974	222.052127	48.062017
1889.966420	219.282006	48.067021
1886.359118	229.826987	48.072026
1882.735737	216.550755	48.077031
1879.538803	218.271087	48.082036
1876.211207	211.607942	48.087041
1872.853783	226.095151	48.092045
1869.104932	227.750766	48.097050
1865.355008	214.870122	48.102055
1861.895555	208.736327	48.107060
1858.320129	212.444195	48.112065
1855.172664	208.431345	48.117069
1851.564754	208.910421	48.122074
1847.944683	216.191004	48.127079
1844.354799	209.198821	48.132084
1840.663721	226.631524	48.137089
1838.002860	219.176380	48.142093
1834.478731	209.162460	48.147098
1830.797337	206.324216	48.152103
1826.971036	206.247596	48.157108
1823.456718	210.257743	48.162113
1819.924436	204.700501	48.167117
1816.167459	214.564703	48.172122
1812.616320	210.788066	48.177127
1809.167194	207.760370	48.182132
1806.125000	216.188892	48.187137
1802.969738	211.541808	48.192141
1798.628791	206.828918	48.197146
1795.375249	200.639287	48.202151
1792.213132	204.528788	48.207156
1788.254830	210.266276	48.212161
1784.986517	209.709105	48.217165
1781.414944	214.391196	48.222170
1778.062749	209.051395	48.227175
1774.324130	208.782064	48.232180
1770.663169	212.879176	48.237185
1767.616542	212.890692	48.242189
1763.756804	217.152213	48.247194
1760.485736	204.974685	48.252199
1756.856487	200.917958	48.257204
1753.265899	202.541203	48.262209
1750.038062	196.868162	48.267213
1746.396690	197.542528	48.272218
1742.871163	205.225359	48.277223
1739.291818	221.363239	48.282228
1735.767520	207.189168	48.287233
1732.580066	205.151267	48.292237
1728.800075	214.166913	48.297242
1725.653597	200.353552	48.302247
1722.048350	194.865825	48.307252
1718.364205	212.854223	48.312257
1715.031329	192.358569	48.317261
1711.452843	208.161168	48.322266
1708.351851	207.468888	48.327271
1704.280737	200.434158	48.332276
1700.697431	197.445334	48.337281
1697.661014	199.010016	48.342285
1694.014749	210.643549	48.347290
1690.365769	199.434977	48.352295
1686.739998	193.603880	48.357300
1683.098915	206.703477	48.362305
1680.183005	193.510338	48.367309
1676.127628	215.406808	48.372314
1672.638900	211.320131	48.377319
1669.470746	199.677364	48.382324
1665.930976	201.505165	48.387329
1662.544313	197.710449	48.392333
1659.046666	202.706746	48.397338
1655.543801	210.930951	48.402343
1651.824074	204.486244	48.407348
1648.442055	211.074227	48.412353
1644.888229	206.496543	48.417357
1641.317749	202.991042	48.422362
1637.743949	201.215139	48.427367
1634.302824	207.029846	48.432372
1630.707835	208.663644	48.437377
1627.492695	199.089088	48.442381
1623.905945	211.091371	48.447386
1620.278013	200.750897	48.452391
1616.889522	199.293570	48.457396
1613.027637	208.564780	48.462401
1610.439424	194.258825	48.467405
1606.496504	204.652203	48.472410
1602.832895	205.234022	48.477415
1599.120734	203.386557	48.482420
1595.988944	206.681268	48.487425
1592.324495	193.994782	48.492429
1588.449722	207.106342	48.497434
1585.367458	198.126878	48.502439
1581.838545	187.001468	48.507444
1578.123435	206.138339	48.512449
1574.793627	193.834082	48.517453
1571.397358	201.531069	48.522458
1567.923779	185.608564	48.527463
1564.179197	202.167683	48.532468
1560.791919	203.718501	48.537473
1557.415368	193.384928	48.542477
1553.887046	195.533400	48.547482
1550.591646	196.624121	48.552487
1546.557173	204.760982	48.557492
1543.157295	196.264393	48.562497
1539.950161	186.964119	48.567501
1536.026995	198.519786	48.572506
1532.639702	202.420210	48.577511
1529.254975	188.737847	48.582516
1525.712679	192.123711	48.587521
1522.264062	196.547861	48.592525
1518.497028	201.900529	48.597530
1515.470989	205.574220	48.602535
1512.167014	197.934827	48.607540
1508.414903	193.209702	48.612545
1504.825034	188.669816	48.617549
1501.179256	196.433755	48.622554
1497.627408	199.359598	48.627559
1494.050115	192.736199	48.632564
1490.694822	199.838465	48.637569
1487.332892	200.707268	48.642573
1483.515631	204.462914	48.647578
1480.416659	191.514873	48.652583
1476.914654	189.746050	48.657588
1472.947120	195.984412	48.662593
1469.859936	190.155317	48.667597
1466.289248	201.035554	48.672602
1462.741176	189.722775	48.677607
1459.246103	187.680034	48.682612
1455.443076	186.600095	48.687617
1452.459901	189.623990	48.692621
1448.596055	179.119639	48.697626
1445.156795	190.282045	48.702631
1442.039053	183.841708	48.707636
1438.297262	200.292183	48.712641
1435.023653	191.206069	48.717645
1431.110313	181.995973	48.722650
1427.528634	187.676012	48.727655
1424.331947	187.928893	48.732660
1420.565994	186.099285	48.737665
1417.257098	196.639574	48.742669
1413.314784	191.945009	48.747674
1409.942302	180.819839	48.752679
1406.409337	185.722134	48.757684
1402.992729	185.368975	48.762689
1400.065362	185.473039	48.767693
1396.593737	197.879729	48.772698
1392.847598	189.061543	48.777703
1388.793211	182.564999	48.782708
1385.628227	195.762022	48.787713
1382.275729	174.154558	48.792717
1378.638607	183.127817	48.797722
1375.419506	178.529771	48.802727
1371.998714	180.288352	48.807732
1367.908634	182.744207	48.812737
1364.653445	174.389496	48.817741
1360.949150	198.353540	48.822746
1357.710003	182.114473	48.827751
1353.991093	177.649741	48.832756
1350.547179	184.768560	48.837761
1347.114533	179.547051	48.842765
1343.358427	175.950223	48.847770
1340.049500	188.956338	48.852775
1336.930880	183.979757	48.857780
1333.142217	179.854778	48.862785
1329.880023	181.252758	48.867789
1325.857974	189.800544	48.872794
1322.596964	192.342542	48.877799
1319.077883	185.157069	48.882804
1315.372404	184.986299	48.887809
1311.876206	185.302580	48.892813
1308.398878	182.175822	48.897818
1305.044571	189.895285	48.902823
1301.632777	188.174902	48.907828
1298.347379	184.687650	48.912833
1295.102493	192.140839	48.917837
1291.210006	191.408029	48.922842
1287.164546	175.938239	48.927847
1284.214010	184.846747	48.932852
1280.454105	188.753834	48.937857
1277.064821	178.272387	48.942861
1273.647548	181.310884	48.947866
1270.006177	193.072411	48.952871
1266.583368	195.763179	48.957876
1263.024784	184.636258	48.962881
1259.710237	183.148654	48.967885
1256.212612	189.439484	48.972890
1252.399153	178.928132	48.977895
1248.710259	189.118724	48.982900
1245.341716	201.173225	48.987905
1241.955726	171.330589	48.992909
1238.548829	177.609110	48.997914
1235.002440	182.820320	49.002919
1231.887280	171.980719	49.007924
1227.966633	181.536346	49.012929
1224.562303	174.910903	49.017933
1220.853154	181.802847	49.022938
1217.668869	186.162286	49.027943
1214.220852	172.135721	49.032948
1210.471241	179.484908	49.037953
1207.155666	178.129008	49.042957
1203.511187	183.196899	49.047962
1200.223349	181.217163	49.052967
1196.395568	169.824166	49.057972
1192.542012	187.469239	49.062977
1189.329739	172.463883	49.067981
1185.936175	180.657398	49.072986
1182.230369	177.174594	49.077991
1178.800028	186.329565	49.082996
1175.252470	191.157229	49.088001
1172.244717	179.857751	49.093005
1168.645870	178.018952	49.098010
1165.237009	173.047460	49.103015
1161.787831	180.416626	49.108020
1158.138806	174.781174	49.113025
1154.510770	176.802359	49.118029
1150.927779	185.032095	49.123034
1147.434469	173.111748	49.128039
1144.029574	173.686908	49.133044
1140.287066	187.142222	49.138049
1136.826020	173.960572	49.143053
1133.261604	182.177480	49.148058
1129.917704	190.506072	49.153063
1126.835645	179.915197	49.158068
1123.128945	182.298330	49.163073
1119.328528	170.564453	49.168077
1116.041791	180.120746	49.173082
1112.409181	182.002026	49.178087
1109.009654	178.913439	49.183092
1104.945803	174.949159	49.188097
1101.848289	164.460404	49.193101
1098.373118	171.720233	49.198106
1094.878351	177.403140	49.203111
1091.462417	175.710680	49.208116
1087.747768	175.002988	49.213121
1084.725529	173.411771	49.218125
1080.840406	184.450411	49.223130
1077.322085	178.484932	49.228135
1074.342078	171.404075	49.233140
1070.267478	175.273148	49.238145
1066.628731	171.779440	49.243149
1063.364845	164.909128	49.248154
1059.965300	173.319142	49.253159
1056.420812	174.815845	49.258164
1053.030188	172.562713	49.263169
1049.627697	168.684421	49.268173
1045.798477	186.485647	49.273178
1042.272010	176.624252	49.278183
1038.998426	155.937312	49.283188
1034.788973	179.528244	49.288193
1031.926801	163.041205	49.293197
1028.165077	174.270809	49.298202
1024.781210	175.379142	49.303207
1021.573988	166.313100	49.308212
1017.923643	170.082657	49.313217
1014.269256	172.531199	49.318221
1010.634853	175.286321	49.323226
1006.838836	172.748636	49.328231
1003.782496	175.142247	49.333236
1000.421190	173.722575	49.338241
997.190409	164.601441	49.343245
993.510949	176.262612	49.348250
989.762748	171.929706	49.353255
986.404642	171.128772	49.358260
982.729158	175.093396	49.363265
979.452126	165.881352	49.368269
975.513397	162.264385	49.373274
972.148892	166.503919	49.378279
968.993478	160.602304	49.383284
965.200104	178.718953	49.388289
961.740400	168.671182	49.393293
958.235444	173.277135	49.398298
954.590441	168.914190	49.403303
951.473860	166.855990	49.408308
948.015890	166.402257	49.413313
944.352371	162.605402	49.418317
940.522789	178.835537	49.423322
937.559996	171.333414	49.428327
933.985610	176.343886	49.433332
930.114207	178.647667	49.438337
926.761145	167.656431	49.443341
922.904338	170.666742	49.448346
919.734955	167.733326	49.453351
916.292291	164.473699	49.458356
912.679788	169.067637	49.463361
909.504994	174.610681	49.468365
905.727554	170.830091	49.473370
901.773258	166.608221	49.478375
898.929142	175.682189	49.483380
894.890054	179.083001	49.488385
891.743649	172.304469	49.493389
888.060587	175.780076	49.498394
884.717146	174.640753	49.503399
881.611082	165.501164	49.508404
877.797411	172.288489	49.513409
874.164150	172.249480	49.518413
870.539453	176.376448	49.523418
866.972721	167.983197	49.528423
863.657724	177.852845	49.533428
860.459780	173.211620	49.538433
856.524865	168.392378	49.543437
852.907815	165.337681	49.548442
849.247792	174.010005	49.553447
846.393562	158.560116	49.558452
842.771738	172.211368	49.563457
839.330298	157.481654	49.568461
836.132130	176.179103	49.573466
832.099120	180.254538	49.578471
829.009571	180.427852	49.583476
824.759562	177.022396	49.588481
821.262554	168.635910	49.593485
818.104916	168.581135	49.598490
814.861067	164.554740	49.603495
811.391474	171.948043	49.608500
807.470344	169.584842	49.613505
803.866104	160.531808	49.618509
800.554563	175.952421	49.623514
797.147974	170.700876	49.628519
793.948064	170.065307	49.633524
789.971079	179.848868	49.638529
786.399575	168.310247	49.643533
783.196195	168.892955	49.648538
779.773501	183.895093	49.653543
776.340894	168.732039	49.658548
772.415216	176.531568	49.663553
769.253438	162.799384	49.668557
765.879237	169.930316	49.673562
762.012164	169.251431	49.678567
758.574520	162.248587	49.683572
754.947588	167.742153	49.688577
751.536971	164.474464	49.693581
747.733528	163.075554	49.698586
744.532206	157.752459	49.703591
741.360109	161.060393	49.708596
737.191127	174.080290	49.713601
733.927955	163.544127	49.718605
730.918260	167.510306	49.723610
727.303055	168.142209	49.728615
723.880117	159.472058	49.733620
720.118300	159.160866	49.738625
716.527685	164.127949	49.743629
713.328669	159.545585	49.748634
709.443493	153.215321	49.753639
705.971928	158.398039	49.758644
702.385802	162.297829	49.763649
698.938619	152.577673	49.768653
695.625003	162.091795	49.773658
691.925785	169.291826	49.778663
688.491597	165.394502	49.783668
684.731226	165.166553	49.788673
681.704425	156.204100	49.793677
678.035674	157.330255	49.798682
674.347503	164.403077	49.803687
671.030111	163.650631	49.808692
667.629194	175.762170	49.813697
664.079576	163.248170	49.818701
660.539926	151.788340	49.823706
656.821621	166.402189	49.828711
653.194177	159.489850	49.833716
649.836739	169.311438	49.838721
646.724216	162.776157	49.843725
643.207011	165.979734	49.848730
639.434959	167.434325	49.853735
636.250117	148.165298	49.858740
632.311234	167.560090	49.863745
628.933479	164.808233	49.868749
625.311518	158.807958	49.873754
621.971967	164.640555	49.878759
618.479308	156.116057	49.883764
614.913314	162.548881	49.888769
611.539700	156.439920	49.893773
607.777137	161.718200	49.898778
604.572965	159.621760	49.903783
601.252141	158.373190	49.908788
597.658314	155.053570	49.913793
593.864497	161.940256	49.918797
590.411564	169.952529	49.923802
586.739891	157.714261	49.928807
583.460745	163.289175	49.933812
579.663365	165.775571	49.938817
576.464978	155.535132	49.943821
572.993570	159.982021	49.948826
569.398668	174.410284	49.953831
566.200353	163.704479	49.958836
562.370787	159.230586	49.963841
559.029774	158.195113	49.968845
555.624536	164.913261	49.973850
552.063169	159.223453	49.978855
548.619534	150.553479	49.983860
544.755137	156.780995	49.988865
541.582768	149.627726	49.993869
537.501166	142.330260	49.998874
533.872400	155.293864	50.003879
530.960566	154.908484	50.008884
527.838185	152.093983	50.013889
524.196583	142.798801	50.018893
520.423815	148.113830	50.023898
516.164395	156.523046	50.028903
513.316244	159.670533	50.033908
509.687720	163.248312	50.038913
506.243999	150.689413	50.043917
502.813540	153.574084	50.048922
499.434271	154.355175	50.053927
495.981928	158.054603	50.058932
492.296598	159.591534	50.063937
489.072203	154.001190	50.068941
485.445079	151.254104	50.073946
481.528916	145.058745	50.078951
478.418654	155.366183	50.083956
474.926822	152.681893	50.088961
471.361572	142.397849	50.093965
467.864325	150.538437	50.098970
464.351434	147.863553	50.103975
460.719471	150.988507	50.108980
456.828900	153.669126	50.113985
453.988053	160.365612	50.118989
450.558671	156.770501	50.123994
446.497125	157.750941	50.128999
443.048800	152.788061	50.134004
439.225123	164.981947	50.139009
436.112194	136.564007	50.144013
432.609202	148.233046	50.149018
429.056404	158.385813	50.154023
426.113666	146.749799	50.159028
422.419649	159.049534	50.164033
419.014955	157.617210	50.169037
415.289149	151.967182	50.174042
411.621470	156.439764	50.179047
408.666966	154.747015	50.184052
404.730182	160.151849	50.189057
401.439227	153.081780	50.194061
397.760136	150.933778	50.199066
394.112521	164.186364	50.204071
391.073197	147.735607	50.209076
387.171260	159.589752	50.214081
383.646536	154.732854	50.219085
380.165491	152.379796	50.224090
376.373372	160.192973	50.229095
373.224383	143.595695	50.234100
369.627089	153.959953	50.239105
366.317210	151.745351	50.244109
362.852525	151.725244	50.249114
358.740223	149.903558	50.254119
356.122737	150.936325	50.259124
352.354427	162.241894	50.264129
348.613878	144.905868	50.269133
345.142284	153.170426	50.274138
342.041164	143.718694	50.279143
338.413366	142.978536	50.284148
334.653644	149.546095	50.289153
331.262738	146.500320	50.294157
327.582787	149.042234	50.299162
324.004071	154.318600	50.304167
320.481387	150.247483	50.309172
316.677378	158.201461	50.314177
313.618527	146.023746	50.319181
310.235174	147.855981	50.324186
306.473998	158.036520	50.329191
303.363281	157.614845	50.334196
299.591189	151.572198	50.339201
296.331636	147.846322	50.344205
292.652594	144.696343	50.349210
288.823635	150.227853	50.354215
285.825273	138.585628	50.359220
282.190346	154.763525	50.364225
278.822720	160.922921	50.369229
275.444088	141.587221	50.374234
271.575037	150.159772	50.379239
268.041108	154.345740	50.384244
264.445522	149.270266	50.389249
261.132599	149.443757	50.394253
257.779980	149.501774	50.399258
253.718834	154.660869	50.404263
250.798141	151.466222	50.409268
247.047396	151.327503	50.414273
243.625511	156.692339	50.419277
240.065285	163.329493	50.424282
236.372122	151.380927	50.429287
233.372276	153.622096	50.434292
229.777904	153.569326	50.439297
226.387922	151.455443	50.444301
222.274992	153.441809	50.449306
218.980505	158.768936	50.454311
215.621888	144.828728	50.459316
211.845158	156.255122	50.464321
208.309738	160.398157	50.469325
205.116935	142.510731	50.474330
201.612062	146.196095	50.479335
198.123733	149.250398	50.484340
194.087853	145.312098	50.489345
191.012578	145.167070	50.494349
188.026475	154.672957	50.499354
184.149278	159.043937	50.504359
180.731493	141.529916	50.509364
177.228113	152.988404	50.514369
173.380275	152.772050	50.519373
169.701210	144.847484	50.524378
166.344908	148.230112	50.529383
163.308489	149.973528	50.534388
159.487067	151.970070	50.539393
156.028516	145.446765	50.544397
152.636496	142.070389	50.549402
149.201498	153.994090	50.554407
145.659492	138.711958	50.559412
141.894239	143.879344	50.564417
138.381567	159.100775	50.569421
135.162464	149.445007	50.574426
131.268303	144.213160	50.579431
128.220900	148.503190	50.584436
124.568236	156.923554	50.589441
121.060068	146.499987	50.594445
117.595105	143.992298	50.599450
113.549137	154.856996	50.604455
110.563640	145.491951	50.609460
106.880639	147.499391	50.614465
103.241863	145.485289	50.619469
100.074659	148.575171	50.624474
96.182703	147.133964	50.629479
93.024940	136.918985	50.634484
89.161475	143.576717	50.639489
85.847853	144.826534	50.644493
82.771465	155.873065	50.649498
79.007772	138.063791	50.654503
75.596105	147.582227	50.659508
71.828024	153.294987	50.664513
68.588487	144.197865	50.669517
65.220375	139.854134	50.674522
61.494859	142.832671	50.679527
57.972586	145.193593	50.684532
54.690373	148.065732	50.689537
50.431529	139.754737	50.694541
47.308256	135.815389	50.699546
43.900945	144.649839	50.704551
40.449211	138.065697	50.709556
36.542000	137.815535	50.714561
33.301125	139.759522	50.719565
30.075563	138.263482	50.724570
26.175099	140.622398	50.729575
23.188782	135.781916	50.734580
19.336875	151.305687	50.739585
15.830899	133.653259	50.744589
12.327278	137.962300	50.749594
8.850090	146.614065	50.754599
5.659638	136.108185	50.759604
1.375626	147.008921	50.764609