Thu Jun 16 11:41:07 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
1.063057	75.711310	0.000000
0.528300	94.097041	0.005005
0.513068	66.398898	0.010010
-0.130947	65.220739	0.015014
-0.419047	68.594330	0.020019
-0.007175	48.839360	0.025024
-0.417726	52.956412	0.030029
-0.556546	44.029103	0.035034
-1.125537	35.645144	0.040038
-1.035961	31.697407	0.045043
-1.768539	17.013367	0.050048
-1.970504	13.606982	0.055053
-1.737987	14.951157	0.060058
-2.124712	25.495563	0.065062
-2.890674	7.690729	0.070067
-2.645721	-5.651658	0.075072
-3.026619	4.697819	0.080077
-3.259001	-3.771442	0.085082
-3.750061	-10.972284	0.090086
-4.083731	-6.958812	0.095091
-4.180727	-1.244410	0.100096
-4.829693	-9.278819	0.105101
-5.357880	-18.724487	0.110106
-5.530209	-3.087947	0.115110
-5.629960	-21.651388	0.120115
-5.821560	-28.606048	0.125120
-5.814172	0.536170	0.130125
-5.745089	-8.172125	0.135130
-5.720059	-10.234481	0.140134
-6.493353	-11.469994	0.145139
-7.098210	-11.516064	0.150144
-7.487785	-4.628174	0.155149
-7.333046	-12.365769	0.160154
-7.208191	-14.146295	0.165158
-7.848211	-11.742033	0.170163
-8.246030	-13.780480	0.175168
-9.062493	-13.846332	0.180173
-9.151576	-11.486060	0.185178
-8.911178	-8.351653	0.190182
-8.933500	-8.360318	0.195187
-8.739654	-13.654722	0.200192
-9.248024	0.601462	0.205197
-9.732330	-5.298180	0.210202
-9.805110	-9.097436	0.215206
-10.252828	-5.853846	0.220211
-10.302046	-12.105661	0.225216
-11.242520	-12.553818	0.230221
-11.838917	-18.679392	0.235226
-11.932174	-12.549395	0.240230
-12.056992	-4.315634	0.245235
-11.866581	-24.229441	0.250240
-12.271625	-6.035345	0.255245
-12.522226	-9.577720	0.260250
-12.038613	-16.275897	0.265254
-12.379127	0.049907	0.270259
-12.981303	-10.419492	0.275264
-13.560938	-7.727275	0.280269
-13.272924	-7.057195	0.285274
-13.480454	-21.190569	0.290278
-14.243304	-9.425152	0.295283
-14.588313	-15.692503	0.300288
-14.871901	-10.487097	0.305293
-15.212032	-12.314194	0.310298
-15.209309	-2.638585	0.315302
-15.423214	-10.626705	0.320307
-15.001354	-16.796847	0.325312
-16.086411	-8.485983	0.330317
-16.209036	-1.332044	0.335322
-16.328908	-9.538239	0.340326
-16.791847	-11.657474	0.345331
-16.393671	-7.841504	0.350336
-17.315748	-3.826384	0.355341
-17.879868	-23.021111	0.360346
-18.360728	-17.480241	0.365350
-18.445750	-8.159689	0.370355
-17.480263	-14.870912	0.375360
-18.061912	-6.226334	0.380365
-18.258747	-19.613488	0.385370
-18.719435	-15.224370	0.390374
-19.440383	-6.495606	0.395379
-19.797814	-10.227299	0.400384
-19.830240	-2.918387	0.405389
-19.876088	-15.869689	0.410394
-19.557551	-11.914184	0.415398
-20.243534	-7.886290	0.420403
-20.682302	-25.834235	0.425408
-21.046564	-16.336134	0.430413
-21.605726	-8.499788	0.435418
-21.699127	-13.971058	0.440422
-21.809620	-4.095219	0.445427
-21.675671	-16.794974	0.450432
-21.691455	-4.650577	0.455437
-22.280138	-12.178693	0.460442
-22.640514	-7.604109	0.465446
-23.107735	-1.611586	0.470451
-22.883357	-16.427890	0.475456
-23.420076	-8.383643	0.480461
-23.640283	-13.839184	0.485466
-24.460211	-16.855072	0.490470
-24.681616	-6.108642	0.495475
-24.722157	-14.631104	0.500480
-24.894607	-7.094546	0.505485
-24.773092	-15.342405	0.510490
-24.736191	-12.700879	0.515494
-24.932107	-6.689465	0.520499
-25.166383	-17.036853	0.525504
-25.833271	-8.982833	0.530509
-25.737082	-16.577271	0.535514
-26.524220	-20.351693	0.540518
-27.153783	-7.788103	0.545523
-27.309456	-27.905644	0.550528
-27.838892	-15.212305	0.555533
-27.910257	-5.480456	0.560538
-27.635620	-10.789792	0.565542
-27.999095	-10.453813	0.570547
-27.791882	-13.336289	0.575552
-28.057649	-11.765539	0.580557
-28.505079	-7.607090	0.585562
-28.851617	-7.676808	0.590566
-29.484554	-6.929801	0.595571
-29.520575	-19.742832	0.600576
-29.515046	-2.172792	0.605581
-29.657386	-12.441952	0.610586
-30.253455	-12.253001	0.615590
-30.796529	-5.731692	0.620595
-31.025642	-12.061702	0.625600
-31.294219	-19.650607	0.630605
-31.473316	-10.662854	0.635610
-31.200783	-1.925829	0.640614
-31.348475	-11.433984	0.645619
-31.046999	-17.462296	0.650624
-31.861830	-11.205354	0.655629
-32.584363	-21.724894	0.660634
-32.472929	-8.633348	0.665638
-32.995978	-11.345811	0.670643
-33.810407	-18.789360	0.675648
-33.756987	-17.525589	0.680653
-34.180281	-10.597897	0.685658
-34.277291	-10.272413	0.690662
-34.536296	-8.062127	0.695667
-34.370185	-25.714732	0.700672
-34.333049	-22.474128	0.705677
-34.321669	-17.925569	0.710682
-34.579370	-16.732809	0.715686
-35.645501	-15.811018	0.720691
-35.510924	-14.134874	0.725696
-35.931327	-19.252292	0.730701
-36.182229	-16.850973	0.735706
-36.707718	-16.168879	0.740710
-37.321500	-13.076901	0.745715
-37.208688	-24.771235	0.750720
-37.747448	-11.329551	0.755725
-37.138266	-12.456734	0.760730
-36.978935	-21.759223	0.765734
-37.980463	-16.415734	0.770739
-37.700027	-17.432453	0.775744
-38.564141	-12.847623	0.780749
-38.828434	-17.317831	0.785754
-38.867752	-12.027703	0.790758
-38.983180	-7.443288	0.795763
-39.178386	-12.391938	0.800768
-40.160900	-12.826336	0.805773
-40.767145	-9.628761	0.810778
-40.633317	-18.328608	0.815782
-40.715012	-21.065473	0.820787
-40.268118	-17.317836	0.825792
-40.976937	-15.638941	0.830797
-41.094017	-14.623714	0.835802
-40.899409	-12.495498	0.840806
-41.587160	-15.248515	0.845811
-42.029010	-12.778052	0.850816
-42.224337	-15.940570	0.855821
-42.520644	-9.612759	0.860826
-42.299779	-15.947681	0.865830
-43.105710	-8.390582	0.870835
-43.339845	-9.962912	0.875840
-43.345346	-10.521881	0.880845
-43.663754	-11.296980	0.885850
-44.038684	-10.810141	0.890854
-44.247329	-8.492458	0.895859
-44.576139	-11.722986	0.900864
-45.064917	-11.010457	0.905869
-45.146333	-10.651049	0.910874
-45.238048	-9.388053	0.915878
-45.813657	-10.392039	0.920883
-45.269592	0.802145	0.925888
-45.538729	-11.655194	0.930893
-46.357423	-9.028533	0.935898
-46.453009	-11.807103	0.940902
-47.027838	0.715977	0.945907
-47.340670	-17.126804	0.950912
-47.231055	-9.284279	0.955917
-47.516890	-13.696076	0.960922
-47.314863	-15.149793	0.965926
-47.902784	-10.912781	0.970931
-48.561407	-12.689508	0.975936
-48.647773	-15.373217	0.980941
-48.938686	-20.717330	0.985946
-48.916885	-7.030498	0.990950
-49.440731	-10.056841	0.995955
-48.979238	-15.678118	1.000960
-49.432003	-12.622220	1.005965
-50.324888	-14.852114	1.010970
-50.505528	-15.642384	1.015974
-50.833572	-10.426277	1.020979
-50.429063	-9.936059	1.025984
-50.623891	-19.911726	1.030989
-51.117049	-20.207889	1.035994
-51.587990	-13.894035	1.040998
-51.909084	-14.410909	1.046003
-52.016412	-16.332216	1.051008
-52.317057	-11.716501	1.056013
-52.109724	-5.877290	1.061018
-52.434456	-21.655265	1.066022
-53.719242	-11.428009	1.071027
-54.090429	-9.547230	1.076032
-54.074411	-13.306505	1.081037
-53.676354	-17.116388	1.086042
-53.715219	-10.587650	1.091046
-54.379156	-20.578324	1.096051
-54.073952	-12.501664	1.101056
-54.397810	-15.855043	1.106061
-55.372168	-7.737579	1.111066
-55.270550	-15.272636	1.116070
-55.810888	-18.530058	1.121075
-55.412466	-7.877093	1.126080
-55.827739	-13.341531	1.131085
-56.028672	-20.449236	1.136090
-56.373152	-13.964106	1.141094
-57.012553	-7.101618	1.146099
-57.004528	-10.257592	1.151104
-57.087338	-13.528380	1.156109
-57.579520	-9.522648	1.161114
-57.490196	-21.761117	1.166118
-58.310876	-8.367349	1.171123
-58.822486	-15.188719	1.176128
-58.566130	-12.689811	1.181133
-58.994327	-11.663810	1.186138
-58.928861	-9.168375	1.191142
-59.119209	-21.442308	1.196147
-58.946609	-19.238342	1.201152
-59.823384	-7.770082	1.206157
-60.264335	-9.147526	1.211162
-60.407932	-11.716711	1.216166
-60.626292	-15.741988	1.221171
-60.531370	-15.052922	1.226176
-60.775549	-17.349577	1.231181
-61.435306	-11.260915	1.236186
-61.643664	-20.530751	1.241190
-62.411736	-12.351492	1.246195
-62.323871	-16.632675	1.251200
-62.351773	-20.320663	1.256205
-62.355122	-17.108981	1.261210
-62.220347	-25.032286	1.266214
-62.727672	-17.234304	1.271219
-63.295244	-9.230733	1.276224
-64.092734	-6.962626	1.281229
-64.279446	-21.221661	1.286234
-64.128887	-18.227099	1.291238
-64.297401	-19.471893	1.296243
-64.153445	-25.648389	1.301248
-64.241826	-15.359802	1.306253
-64.710422	-7.751020	1.311258
-64.914285	-16.793811	1.316262
-65.360863	-8.666401	1.321267
-65.048906	-16.284460	1.326272
-66.358368	-10.708553	1.331277
-66.492235	-0.529046	1.336282
-66.472493	-29.106644	1.341286
-66.885064	-5.706981	1.346291
-67.053045	-10.631717	1.351296
-67.068906	-20.418443	1.356301
-67.729944	-13.628740	1.361306
-67.844959	-16.992265	1.366310
-68.328086	-6.843828	1.371315
-68.216761	-23.026622	1.376320
-68.453248	-15.229501	1.381325
-68.594211	-8.356953	1.386330
-68.842941	-19.719352	1.391334
-69.317127	-5.857915	1.396339
-69.713208	-15.741819	1.401344
-69.684831	-12.982278	1.406349
-69.662609	-7.608601	1.411354
-70.384938	-5.727402	1.416358
-71.212163	-11.723565	1.421363
-71.225739	-13.468289	1.426368
-71.560761	-6.566925	1.431373
-71.665621	-10.292706	1.436378
-71.153156	-21.013387	1.441382
-71.609415	-10.975149	1.446387
-71.327883	-27.796137	1.451392
-71.871379	-21.717322	1.456397
-72.750635	-10.861484	1.461402
-73.148536	-32.676449	1.466406
-73.131984	-7.527963	1.471411
-73.158111	-15.819981	1.476416
-73.112495	-24.800610	1.481421
-73.991942	-2.144080	1.486426
-74.334803	-14.993803	1.491430
-74.785781	-21.572144	1.496435
-74.523631	-20.858924	1.501440
-74.753553	-16.604229	1.506445
-74.852807	-5.813078	1.511450
-74.826119	-12.318935	1.516454
-75.894154	-12.923674	1.521459
-76.284613	-16.601759	1.526464
-76.761779	-11.934377	1.531469
-76.189808	-15.373855	1.536474
-76.162298	-22.487447	1.541478
-76.397097	-8.923653	1.546483
-76.426152	-3.831244	1.551488
-77.090800	-9.093070	1.556493
-77.884099	-10.199978	1.561498
-77.647130	-7.769489	1.566502
-77.878675	4.701988	1.571507
-78.403173	-10.941561	1.576512
-79.166348	-17.097470	1.581517
-79.468579	-15.758544	1.586522
-78.685160	-10.765395	1.591526
-79.421733	-11.849813	1.596531
-79.632821	-16.948745	1.601536
-79.658429	-19.955125	1.606541
-79.614649	-21.363451	1.611546
-80.144861	-19.073420	1.616550
-80.918948	-16.992773	1.621555
-81.300063	-13.402080	1.626560
-81.283260	-11.322712	1.631565
-81.538851	-12.580935	1.636570
-81.601978	-26.163504	1.641574
-81.434863	-15.045153	1.646579
-81.697814	-13.458786	1.651584
-82.302706	-15.919865	1.656589
-82.970083	-23.402601	1.661594
-82.913998	-1.914939	1.666598
-83.145915	-12.516052	1.671603
-83.061248	-16.760007	1.676608
-83.118503	-16.550893	1.681613
-83.981913	-13.001636	1.686618
-84.254786	-22.897905	1.691622
-84.785130	-7.602840	1.696627
-84.592185	-13.577601	1.701632
-84.607689	-10.481406	1.706637
-84.709391	-12.908055	1.711642
-85.040967	-11.188115	1.716646
-85.659278	-2.886017	1.721651
-86.183435	-0.155216	1.726656
-86.294164	-7.755903	1.731661
-86.099996	-10.153319	1.736666
-86.007215	-15.510137	1.741670
-87.299195	-1.346518	1.746675
-87.504917	-2.419032	1.751680
-87.741937	-16.781427	1.756685
-87.938512	-11.260903	1.761690
-88.093963	-21.396476	1.766694
-88.354239	-6.272617	1.771699
-87.889457	-17.356947	1.776704
-88.211078	-20.805101	1.781709
-88.440517	-11.503998	1.786714
-88.899347	-15.713273	1.791718
-89.423391	-17.612074	1.796723
-89.491228	-12.231408	1.801728
-89.461812	-13.927400	1.806733
-90.036855	-16.198769	1.811738
-90.344874	-10.533155	1.816742
-90.998352	-9.949470	1.821747
-90.887934	-6.563527	1.826752
-90.837429	-4.106462	1.831757
-91.136719	1.756302	1.836762
-91.489057	-17.769371	1.841766
-92.263812	-18.112907	1.846771
-92.384118	-15.350991	1.851776
-92.684169	-17.597370	1.856781
-92.766248	-16.837617	1.861786
-92.722972	-5.345419	1.866790
-92.923877	-4.118735	1.871795
-92.701478	-16.072190	1.876800
-93.819633	-22.363573	1.881805
-94.164608	-14.373907	1.886810
-94.222795	-23.291209	1.891814
-94.471158	-10.867379	1.896819
-94.589140	-9.067218	1.901824
-94.531125	-10.960014	1.906829
-94.819302	-4.032849	1.911834
-95.485460	-11.370375	1.916838
-95.795372	-11.767160	1.921843
-95.882344	-7.105074	1.926848
-95.880331	-12.976361	1.931853
-96.163266	-12.389695	1.936858
-96.548292	-19.435499	1.941862
-97.629848	-10.207835	1.946867
-97.730859	-5.042469	1.951872
-97.868437	-19.558916	1.956877
-97.487836	-10.175143	1.961882
-97.415499	-13.320928	1.966886
-97.940524	0.365519	1.971891
-97.706232	-10.764082	1.976896
-98.324452	-10.518487	1.981901
-99.042091	3.613943	1.986906
-99.429381	-10.856900	1.991910
-99.379912	-10.347270	1.996915
-99.556902	-14.896461	2.006912
-99.583175	-1.853064	2.016909
-98.905380	-3.668926	2.026906
-98.110369	-4.880865	2.036902
-97.915904	-9.562046	2.046899
-97.434045	-9.468670	2.056896
-96.713458	-10.521522	2.066893
-96.471001	-3.455760	2.076890
-95.939616	-2.571742	2.086886
-95.086811	0.492256	2.096883
-94.762677	-4.214506	2.106880
-94.602305	-3.944473	2.116877
-93.497697	-9.026532	2.126874
-93.553463	-10.806401	2.136870
-92.977972	-3.791088	2.146867
-91.960070	-16.977873	2.156864
-92.006077	-10.509021	2.166861
-91.527425	-16.728487	2.176858
-90.850724	-26.116821	2.186854
-90.450519	-23.212229	2.196851
-89.421667	-17.453694	2.206848
-88.953034	-19.999338	2.216845
-88.972497	-9.918667	2.226842
-88.711354	-13.869380	2.236838
-87.929480	-20.059986	2.246835
-87.287531	-13.565904	2.256832
-86.304348	-14.089680	2.266829
-86.196980	-14.446926	2.276826
-85.971273	-13.012663	2.286822
-85.765565	-13.912309	2.296819
-84.788680	-21.518843	2.306816
-84.577596	-12.644142	2.316813
-83.455679	-11.537036	2.326810
-83.318695	-15.489109	2.336806
-82.939353	-19.662791	2.346803
-82.338754	-21.197361	2.356800
-81.665185	-9.466144	2.366797
-81.692593	-15.504675	2.376794
-80.347359	-13.571740	2.386790
-80.091192	-22.442610	2.396787
-79.956096	-16.169936	2.406784
-79.487428	-12.332081	2.416781
-78.842426	-18.413189	2.426778
-78.116373	-11.950538	2.436774
-77.839427	-13.262853	2.446771
-77.000882	-15.653751	2.456768
-76.989924	-14.230670	2.466765
-76.288394	-20.194089	2.476762
-75.461681	-17.764288	2.486758
-75.161275	-13.019933	2.496755
-75.110401	-18.960077	2.506752
-74.304464	-15.759870	2.516749
-73.719180	-16.442951	2.526746
-73.459031	-7.973300	2.536742
-72.341699	-19.327713	2.546739
-72.127728	-14.162942	2.556736
-71.956579	-13.231042	2.566733
-71.357046	-16.932997	2.576730
-70.727726	-15.206327	2.586726
-70.498905	-19.418747	2.596723
-69.338775	-11.113988	2.606720
-69.014166	-6.227881	2.616717
-68.956655	-8.782183	2.626714
-68.550477	-12.289444	2.636710
-67.487108	-9.989530	2.646707
-67.185653	-5.852344	2.656704
-66.874909	-8.110870	2.666701
-66.294092	-11.905647	2.676698
-65.951842	-8.459052	2.686694
-65.248708	-7.825670	2.696691
-64.588976	-14.384934	2.706688
-64.626384	-14.235370	2.716685
-63.565206	-19.458760	2.726682
-63.073825	-9.964460	2.736678
-62.784876	-9.587510	2.746675
-62.428174	-13.308155	2.756672
-61.521228	-6.902361	2.766669
-61.511298	-15.439611	2.776666
-60.798630	-9.064385	2.786662
-59.787957	-13.248322	2.796659
-59.661288	-9.223355	2.806656
-59.410039	-8.355662	2.816653
-58.509814	-9.982521	2.826650
-57.937669	-8.275195	2.836646
-57.995066	-12.723513	2.846643
-57.755081	-8.544854	2.856640
-56.615457	-14.479727	2.866637
-56.040437	-7.518413	2.876634
-55.316620	-10.159670	2.886630
-55.045689	-8.703049	2.896627
-54.579462	-17.701047	2.906624
-54.803854	-2.414173	2.916621
-53.769635	-5.419071	2.926618
-53.414047	-4.861897	2.936614
-52.127951	-13.790429	2.946611
-51.987712	-5.355383	2.956608
-51.623191	-17.368108	2.966605
-51.299828	-7.981216	2.976602
-51.018212	-4.784091	2.986598
-50.214686	-7.678309	2.996595
-49.975073	-9.960047	3.006592
-48.485163	-6.677685	3.016589
-48.557679	-7.104524	3.026586
-48.443069	-3.036914	3.036582
-48.085934	-12.487421	3.046579
-47.090885	-16.886878	3.056576
-46.654468	-11.727999	3.066573
-46.448469	-7.235728	3.076570
-45.412559	-4.084338	3.086566
-45.424931	-7.953302	3.096563
-44.353693	-9.036095	3.106560
-43.787358	-7.093650	3.116557
-43.626845	-11.125229	3.126554
-43.673591	-16.038088	3.136550
-42.653761	-12.179301	3.146547
-41.800012	-13.341772	3.156544
-41.734529	-10.679625	3.166541
-41.578354	-6.535367	3.176538
-40.707281	-11.214575	3.186534
-40.228002	-14.647236	3.196531
-39.357967	-15.503021	3.206528
-39.050011	-5.458130	3.216525
-39.158361	-11.444271	3.226522
-38.204420	-5.005442	3.236518
-37.580145	-3.449711	3.246515
-37.229288	-8.154912	3.256512
-36.895954	-4.553090	3.266509
-36.019663	-4.620119	3.276506
-35.820844	-7.472381	3.286502
-35.217211	-8.871925	3.296499
-34.448545	-13.242315	3.306496
-34.285040	-10.272865	3.316493
-33.621388	-5.626812	3.326490
-32.654873	-11.151539	3.336486
-32.702664	-8.404538	3.346483
-32.391092	-13.101714	3.356480
-31.343456	-13.185651	3.366477
-31.171260	1.585847	3.376474
-30.860340	-4.040984	3.386470
-30.454719	2.074977	3.396467
-29.532480	-2.909175	3.406464
-29.299647	-2.556929	3.416461
-28.233119	-10.430808	3.426458
-27.867772	-11.138039	3.436454
-27.646490	-17.285732	3.446451
-27.606833	-4.289623	3.456448
-26.256720	-14.220624	3.466445
-26.063358	-10.707142	3.476442
-25.932554	-10.029646	3.486438
-25.141591	-7.790942	3.496435
-24.570104	-9.718531	3.506432
-24.289556	-2.914054	3.516429
-23.292607	-5.500632	3.526426
-23.009368	-6.291098	3.536422
-22.828475	-6.926062	3.546419
-22.281174	-11.243767	3.556416
-21.315740	-7.991083	3.566413
-21.098788	-3.403619	3.576410
-20.970734	-3.353657	3.586406
-19.946767	-2.355948	3.596403
-19.742507	-8.303668	3.606400
-19.177683	-10.989126	3.616397
-18.218480	-9.151660	3.626394
-17.959573	-13.393847	3.636390
-17.879051	-9.658627	3.646387
-17.089356	-14.245014	3.656384
-16.409565	-5.943928	3.666381
-16.127348	-14.451504	3.676378
-16.095498	-4.987931	3.686374
-15.225599	-8.811811	3.696371
-14.716050	-10.306486	3.706368
-13.445383	-13.020185	3.716365
-13.805903	-6.815049	3.726362
-13.504070	-11.748575	3.736358
-12.131713	-8.160267	3.746355
-11.982745	-11.620229	3.756352
-12.056032	-10.903423	3.766349
-11.195958	-11.493076	3.776346
-10.488299	-6.008199	3.786342
-10.397474	-8.115895	3.796339
-9.235780	-9.558964	3.806336
-8.636161	-10.495950	3.816333
-8.566438	-11.997752	3.826330
-8.787315	-14.448014	3.836326
-7.396635	-12.637354	3.846323
-7.300399	-1.333442	3.856320
-6.500782	-15.437867	3.866317
-5.751937	-2.224043	3.876314
-5.473097	-6.549735	3.886310
-5.228274	-1.907261	3.896307
-4.944115	-6.127991	3.906304
-4.338423	-1.519077	3.916301
-3.893305	11.751573	3.926298
-3.506533	23.315186	3.936294
-2.755276	30.493461	3.946291
-2.350988	36.650308	3.956288
-1.724031	56.590278	3.966285
-1.630636	58.919038	3.976282
-1.013789	77.214541	3.986278
-0.387994	94.600849	3.996275
0.115305	111.446153	4.006272
0.000000	108.368676	4.011277
0.433735	118.469855	4.016282
0.401124	137.564152	4.021286
0.543881	123.692591	4.026291
1.160934	153.047671	4.031296
1.366233	159.191338	4.036301
1.460245	156.194947	4.041306
1.279885	168.325344	4.046310
1.375770	152.900696	4.051315
0.806962	155.100642	4.056320
1.105286	153.932976	4.061325
1.608487	155.658122	4.066330
1.485309	149.563287	4.071334
1.299751	138.558004	4.076339
0.938767	141.101842	4.081344
1.133033	138.385538	4.086349
1.289117	150.360187	4.091354
0.943876	154.628266	4.096358
1.675860	154.352783	4.101363
1.286236	161.925118	4.106368
1.198366	168.194879	4.111373
1.731210	158.255398	4.116378
1.548570	166.485291	4.121382
1.453335	152.902628	4.126387
1.067272	153.481183	4.131392
1.393221	162.570552	4.136397
1.426225	144.270573	4.141402
1.387212	150.045592	4.146406
1.375643	154.201999	4.151411
1.218032	159.996523	4.156416
1.357390	154.794231	4.161421
1.529957	170.888925	4.166426
1.097471	155.804639	4.171430
1.859476	149.688613	4.176435
1.809650	163.214599	4.181440
1.837534	159.706367	4.186445
1.800341	159.526626	4.191450
1.411148	152.378620	4.196454
1.486189	147.116126	4.201459
1.094784	151.632055	4.206464
1.205640	160.839740	4.211469
1.635944	156.003910	4.216474
1.485846	152.653343	4.221478
1.963807	158.733305	4.226483
1.948090	163.738825	4.231488
1.520537	163.558976	4.236493
1.553908	163.564981	4.241498
1.329629	164.230844	4.246502
1.645142	167.712371	4.251507
1.439493	174.677478	4.256512
1.667672	171.411881	4.261517
1.779690	170.227648	4.266522
1.534277	172.861997	4.271526
1.664990	161.255716	4.276531
1.783655	167.264144	4.281536
1.641772	163.614775	4.286541
1.766825	161.543758	4.291546
1.510627	175.402387	4.296550
1.581431	173.043187	4.301555
1.825895	167.163032	4.306560
1.737889	172.678902	4.311565
1.659890	168.147661	4.316570
1.550970	175.619058	4.321574
2.154196	189.162434	4.326579
2.193431	205.221979	4.331584
2.087105	184.782967	4.336589
1.744880	159.222373	4.341594
1.418189	188.133667	4.346598
1.893123	188.888982	4.351603
1.864041	187.609090	4.356608
1.939789	205.253992	4.361613
2.097764	191.985690	4.366618
2.245934	199.008255	4.371622
2.039375	191.366669	4.376627
1.541499	198.306780	4.381632
1.917654	195.909051	4.386637
2.035654	200.686890	4.391642
1.867487	196.578773	4.396646
2.077015	191.201008	4.401651
2.234674	191.200975	4.406656
2.473144	190.247215	4.411661
2.656893	182.686646	4.416666
1.962276	195.506999	4.421670
2.424060	203.718809	4.426675
2.112035	192.184980	4.431680
1.832470	189.015818	4.436685
2.173934	187.707048	4.441690
2.334315	194.132608	4.446694
2.529874	193.934824	4.451699
2.402589	179.037046	4.456704
1.928825	165.427745	4.461709
1.774677	167.254522	4.466714
1.994220	194.657207	4.471718
2.242673	178.259647	4.476723
2.162545	190.060862	4.481728
2.220202	190.677173	4.486733
2.147931	187.377271	4.491738
2.015305	179.293636	4.496742
2.110028	191.845424	4.501747
2.512382	197.390364	4.506752
2.458786	181.460814	4.511757
2.421918	199.971267	4.516762
2.004898	192.781177	4.521766
2.336957	190.696664	4.526771
2.357586	194.983805	4.531776
2.406812	190.790634	4.536781
2.317505	194.439892	4.541786
2.413907	194.857623	4.546790
2.417285	194.910808	4.551795
2.521178	186.536416	4.556800
2.161670	198.988460	4.561805
2.093858	187.653710	4.566810
2.649370	193.567758	4.571814
3.009302	194.332806	4.576819
2.691950	193.744962	4.581824
2.722895	200.305269	4.586829
2.643787	199.690582	4.591834
2.183004	191.350313	4.596838
2.699538	194.937925	4.601843
2.472359	195.838868	4.606848
2.571620	184.571219	4.611853
2.398442	203.080427	4.616858
2.439530	194.592006	4.621862
2.567963	195.393436	4.626867
2.475744	205.693664	4.631872
2.419123	190.831254	4.636877
3.050522	203.894179	4.641882
2.470142	207.314031	4.646886
2.631029	190.912776	4.651891
2.714247	209.708533	4.656896
2.426868	217.098555	4.661901
2.774527	212.799727	4.666906
2.706961	223.152914	4.671910
3.018408	216.492757	4.676915
2.777380	225.587763	4.681920
2.718303	213.167536	4.686925
3.103791	221.249507	4.691930
2.699840	210.880279	4.696934
2.870996	211.530418	4.701939
2.678625	204.131045	4.706944
2.930045	205.617036	4.711949
2.899181	205.759836	4.716954
2.677555	216.468181	4.721958
2.655018	214.864605	4.726963
2.999173	217.473152	4.731968
2.883993	220.680775	4.736973
2.735603	214.740134	4.741978
2.737085	215.108242	4.746982
2.954535	223.305293	4.751987
2.956326	201.784501	4.756992
3.143546	218.699404	4.761997
3.429391	217.582531	4.767002
3.281268	217.631157	4.772006
3.419943	211.867122	4.777011
2.944285	208.477412	4.782016
2.814476	188.450705	4.787021
2.604081	190.775809	4.792026
2.681299	204.594261	4.797030
2.690813	205.901317	4.802035
3.048473	213.305688	4.807040
3.014245	215.666301	4.812045
3.395923	216.094501	4.817050
3.460218	218.482340	4.822054
3.547949	225.005058	4.827059
3.055932	216.028189	4.832064
2.991766	222.827775	4.837069
2.962341	225.904025	4.842074
3.094689	227.168092	4.847078
3.297832	206.849271	4.852083
3.171904	216.110030	4.857088
2.845213	216.883877	4.862093
3.119984	211.763268	4.867098
2.910264	224.894577	4.872102
3.150748	210.980643	4.877107
2.850412	222.976122	4.882112
2.895940	217.351782	4.887117
3.084458	203.525860	4.892122
3.086627	225.870606	4.897126
3.286179	236.569541	4.902131
3.036932	243.409983	4.907136
3.483963	246.165992	4.912141
3.626300	250.199421	4.917146
3.481772	251.195623	4.922150
3.490383	229.572051	4.927155
3.524344	237.956985	4.932160
3.365414	243.830188	4.937165
3.518803	223.124752	4.942170
3.343157	219.156080	4.947174
3.519575	222.705791	4.952179
3.252486	231.001764	4.957184
3.111463	237.237718	4.962189
3.785965	238.390091	4.967194
3.752476	242.187885	4.972198
3.695584	232.531385	4.977203
3.213388	232.652485	4.982208
3.368130	237.072165	4.987213
3.822985	232.449787	4.992218
3.554625	250.985142	4.997222
3.801286	235.706461	5.002227
3.500372	224.916600	5.007232
3.033866	227.799998	5.012237
3.562548	231.848696	5.017242
3.558864	244.839426	5.022246
3.744661	242.490808	5.027251
4.027831	251.182520	5.032256
3.566445	251.423203	5.037261
3.780977	245.499524	5.042266
3.203842	247.836805	5.047270
3.527512	247.916180	5.052275
3.277056	253.071213	5.057280
3.416473	237.870038	5.062285
3.574085	252.010179	5.067290
3.727044	254.015981	5.072294
3.578986	246.933049	5.077299
3.744874	248.533018	5.082304
3.484063	255.310363	5.087309
3.759985	243.332856	5.092314
3.593016	252.433299	5.097318
3.763925	265.608583	5.102323
4.066573	266.848949	5.107328
3.578144	255.309992	5.112333
4.094178	262.220394	5.117338
3.757234	259.343641	5.122342
4.055258	261.194851	5.127347
4.187980	257.737837	5.132352
3.987394	252.232587	5.137357
3.904429	246.591884	5.142362
3.890263	255.641032	5.147366
4.089805	243.657601	5.152371
3.903672	245.027377	5.157376
3.852875	254.269627	5.162381
3.747859	244.953637	5.167386
3.618241	256.287961	5.172390
3.888871	264.797861	5.177395
4.090986	267.777846	5.182400
3.762873	273.899415	5.187405
4.222495	270.689863	5.192410
4.058678	279.169854	5.197414
4.182224	286.418205	5.202419
4.242367	279.431569	5.207424
4.005748	278.326154	5.212429
4.375843	278.083840	5.217434
4.365475	277.863557	5.222438
4.337753	258.537404	5.227443
4.008539	255.137294	5.232448
3.954452	249.222392	5.237453
3.939198	242.017578	5.242458
3.901807	270.592258	5.247462
4.387383	273.776476	5.252467
4.349935	274.302060	5.257472
3.924830	280.634404	5.262477
3.978103	269.669172	5.267482
4.026266	275.079311	5.272486
4.340056	287.574454	5.277491
4.222709	274.879877	5.282496
4.202861	274.316461	5.287501
4.530925	285.006327	5.292506
4.002135	276.750747	5.297510
4.315818	271.503328	5.302515
4.080681	286.056756	5.307520
4.070544	286.445432	5.312525
4.071009	277.803265	5.317530
4.285165	289.715449	5.322534
4.032918	268.489201	5.327539
3.961565	275.945559	5.332544
4.401678	297.820359	5.337549
4.843391	314.074349	5.342554
4.585979	294.917517	5.347558
4.280734	285.252699	5.352563
4.292478	276.784670	5.357568
4.225418	312.266421	5.362573
4.608309	301.589618	5.367578
4.344197	305.372266	5.372582
4.701838	310.572735	5.377587
4.661867	309.167762	5.382592
4.643502	308.593543	5.387597
4.858887	294.986157	5.392602
3.927951	283.157454	5.397606
4.507029	296.855663	5.402611
4.701723	304.365835	5.407616
4.404005	297.044401	5.412621
4.533216	301.464669	5.417626
4.555579	304.403335	5.422630
4.636649	311.428161	5.427635
4.575549	303.670337	5.432640
4.440693	306.315639	5.437645
4.632771	296.369838	5.442650
4.473193	318.568902	5.447654
4.617212	310.463947	5.452659
4.745041	303.868922	5.457664
4.704514	297.551220	5.462669
4.920563	305.637067	5.467674
4.619996	306.147139	5.472678
4.697901	299.744161	5.477683
4.959380	306.136290	5.482688
5.021283	299.040931	5.487693
4.977697	298.955080	5.492698
4.762539	309.452680	5.497702
4.904643	306.806824	5.502707
5.331272	313.307315	5.507712
4.719642	312.589729	5.512717
4.860976	304.077973	5.517722
4.556877	299.709744	5.522726
4.860969	303.880125	5.527731
5.180832	306.855655	5.532736
4.943275	299.496555	5.537741
5.034794	306.356082	5.542746
5.027647	307.647845	5.547750
4.827504	307.544557	5.552755
5.175886	304.714459	5.557760
4.844977	309.955416	5.562765
5.180339	299.997969	5.567770
4.828479	308.846057	5.572774
4.662774	307.717872	5.577779
5.307496	312.116780	5.582784
4.837339	309.975308	5.587789
5.199675	314.458373	5.592794
5.017427	322.408893	5.597798
4.976388	313.668991	5.602803
5.038138	315.118464	5.607808
4.921748	312.803398	5.612813
4.859498	311.582743	5.617818
4.845319	319.693425	5.622822
4.954109	315.411749	5.627827
5.227543	313.280970	5.632832
5.090320	320.791841	5.637837
4.999619	314.082576	5.642842
5.108235	319.655091	5.647846
5.101547	315.776956	5.652851
4.890262	315.929052	5.657856
4.924732	320.985720	5.662861
5.211364	317.402136	5.667866
5.176437	346.079249	5.672870
5.338621	328.675591	5.677875
5.519110	335.970493	5.682880
5.397560	339.875403	5.687885
5.480593	322.185512	5.692890
4.997155	325.779181	5.697894
5.456023	318.600947	5.702899
5.543815	323.754365	5.707904
4.875614	322.427265	5.712909
5.378474	322.767469	5.717914
5.208879	334.566316	5.722918
5.741553	334.814382	5.727923
5.350485	338.166869	5.732928
5.307905	333.678264	5.737933
5.145586	331.895236	5.742938
5.376427	344.744889	5.747942
5.250105	341.492361	5.752947
6.044058	342.948888	5.757952
5.269856	345.886708	5.762957
5.669275	337.665934	5.767962
5.358113	345.596138	5.772966
5.552323	334.658375	5.777971
5.544987	330.803134	5.782976
5.518109	347.923839	5.787981
5.605145	340.474477	5.792986
5.378370	340.437249	5.797990
5.770226	330.568016	5.802995
5.627879	343.922401	5.808000
5.617955	343.027834	5.813005
5.840360	337.969209	5.818010
5.516416	345.442680	5.823014
5.466849	343.548677	5.828019
5.222505	342.955470	5.833024
5.425467	332.505888	5.838029
5.649629	334.694580	5.843034
5.493773	346.457525	5.848038
5.504352	345.510044	5.853043
5.354924	339.221766	5.858048
5.166661	344.136093	5.863053
5.379447	341.500550	5.868058
5.386449	361.000563	5.873062
5.646344	368.834829	5.878067
5.729038	358.692488	5.883072
5.532730	369.401688	5.888077
5.646811	383.639415	5.893082
5.531728	367.834173	5.898086
5.750737	375.593414	5.903091
5.860732	365.649491	5.908096
5.490490	374.533014	5.913101
5.919372	360.356562	5.918106
5.824688	373.428834	5.923110
5.584665	373.641814	5.928115
5.929327	373.894315	5.933120
5.703920	368.266058	5.938125
6.099147	382.384711	5.943130
5.818138	384.590006	5.948134
5.728795	372.306948	5.953139
6.151488	388.290489	5.958144
5.869119	385.202450	5.963149
5.858067	383.460813	5.968154
5.912443	398.320972	5.973158
6.177637	397.808016	5.978163
6.227416	389.581166	5.983168
6.020648	398.234061	5.988173
5.876311	384.229663	5.993178
5.904213	389.967373	5.998182
6.322643	392.908281	6.003187
6.354607	398.244386	6.008192
5.943533	383.310141	6.013197
6.134161	371.407699	6.018202
5.641170	379.242085	6.023206
6.090905	393.256932	6.028211
6.323898	400.929918	6.033216
6.081937	407.595200	6.038221
6.399934	393.579008	6.043226
6.151234	393.509887	6.048230
6.069369	384.921813	6.053235
6.105430	374.139791	6.058240
5.673698	376.119902	6.063245
5.991111	379.931265	6.068250
6.069077	397.095767	6.073254
5.689089	407.956103	6.078259
6.007255	399.117723	6.083264
6.025524	400.267472	6.088269
6.464212	397.772266	6.093274
6.443681	405.916008	6.098278
6.285916	387.959214	6.103283
5.991761	381.308501	6.108288
5.939747	396.869331	6.113293
5.948367	388.341182	6.118298
6.153835	407.665702	6.123302
6.270032	407.507174	6.128307
6.364499	393.596094	6.133312
6.043038	398.264501	6.138317
5.886958	371.680708	6.143322
6.006158	398.303797	6.148326
6.181357	404.983403	6.153331
6.373659	394.381540	6.158336
5.779553	392.045076	6.163341
6.311172	386.861442	6.168346
5.981313	389.867212	6.173350
5.749859	390.524503	6.178355
5.995372	395.852052	6.183360
6.149019	404.173297	6.188365
6.096357	406.329908	6.193370
6.466641	405.167695	6.198374
6.393157	392.194371	6.203379
6.078468	384.683814	6.208384
5.846725	382.261818	6.213389
6.086788	384.018047	6.218394
6.132556	385.705362	6.223398
6.180131	377.299823	6.228403
6.152264	363.948829	6.233408
5.865224	374.652506	6.238413
6.253404	376.108713	6.243418
6.172457	381.475705	6.248422
6.241168	392.840494	6.253427
6.154416	377.590530	6.258432
5.886728	370.803151	6.263437
6.419567	375.279365	6.268442
6.015650	368.044605	6.273446
5.793173	373.003958	6.278451
5.971846	371.221991	6.283456
5.959313	380.675627	6.288461
6.062100	388.047817	6.293466
6.310391	407.709667	6.298470
6.225806	396.528971	6.303475
5.955595	376.619141	6.308480
6.042127	386.880084	6.313485
6.424459	381.210383	6.318490
6.182524	382.721000	6.323494
6.014593	384.963151	6.328499
6.423735	374.481934	6.333504
5.762552	378.503360	6.338509
6.208227	371.494601	6.343514
6.087366	374.034311	6.348518
5.977619	384.991739	6.353523
6.258593	376.555422	6.358528
5.982173	377.244215	6.363533
5.972973	390.279289	6.368538
5.812063	389.237221	6.373542
6.050044	385.516243	6.378547
6.095555	386.952029	6.383552
5.817998	397.995998	6.388557
6.264397	401.720740	6.393562
6.431132	411.632425	6.398566
6.148347	411.732310	6.403571
6.271199	383.267405	6.408576
5.961797	385.651914	6.413581
5.966676	378.954942	6.418586
6.040628	380.140276	6.423590
5.759010	369.841881	6.428595
6.215290	388.327496	6.433600
6.084384	388.183168	6.438605
6.148506	401.065254	6.443610
6.221345	402.978360	6.448614
6.034184	386.399416	6.453619
6.013291	390.935871	6.458624
6.237094	404.860505	6.463629
6.187590	377.612401	6.468634
6.148814	375.674879	6.473638
6.326275	381.483270	6.478643
6.003159	375.871847	6.483648
5.871452	380.777332	6.488653
6.153602	374.075975	6.493658
6.125938	376.083526	6.498662
6.046867	375.411605	6.503667
5.825818	365.098962	6.508672
5.855342	387.240632	6.513677
6.277578	388.890792	6.518682
6.425120	403.584518	6.523686
6.014707	388.288191	6.528691
5.852277	375.162359	6.533696
6.034318	395.772665	6.538701
6.435270	382.992246	6.543706
6.119590	385.297092	6.548710
6.099289	374.549147	6.553715
6.375900	374.641134	6.558720
5.937546	380.258385	6.563725
6.034081	375.042378	6.568730
5.869861	379.335948	6.573734
5.827624	379.444027	6.578739
6.029810	395.109252	6.583744
6.123092	393.222317	6.588749
6.518561	402.498736	6.593754
5.994662	385.545699	6.598758
5.879342	376.174112	6.603763
5.957386	385.545795	6.608768
5.940114	408.893698	6.613773
6.396219	400.470059	6.618778
6.365093	406.123314	6.623782
6.107779	400.562569	6.628787
6.039600	382.108650	6.633792
5.701564	391.750750	6.638797
5.970540	402.131508	6.643802
6.032908	407.440691	6.648806
6.481011	410.822326	6.653811
6.440548	402.808088	6.658816
5.917275	390.661740	6.663821
6.119243	381.079670	6.668826
6.213666	387.694778	6.673830
5.776770	381.832235	6.678835
6.137661	382.113328	6.683840
6.064318	412.726419	6.688845
6.007684	400.119473	6.693850
6.233696	398.228064	6.698854
6.326372	408.769767	6.703859
6.174121	388.853055	6.708864
5.891657	382.713715	6.713869
5.968288	387.513247	6.718874
6.220810	401.723376	6.723878
6.157955	389.590422	6.728883
6.073187	390.516478	6.733888
6.061333	388.390908	6.738893
6.439753	369.786839	6.743898
5.888833	381.306405	6.748902
5.747006	387.158191	6.753907
6.163016	389.928133	6.758912
6.268143	389.598887	6.763917
6.317564	383.511839	6.768922
6.164855	385.390592	6.773926
6.318317	377.686555	6.778931
6.211333	380.941395	6.783936
6.207753	386.739553	6.788941
5.932249	377.727893	6.793946
5.955114	382.145140	6.798950
5.876065	379.841257	6.803955
6.132092	375.633294	6.808960
5.455002	385.853112	6.813965
6.196520	393.222844	6.818970
6.360486	396.779289	6.823974
5.987838	399.395536	6.828979
5.725818	387.538289	6.833984
5.829997	406.866919	6.838989
6.540536	381.568032	6.843994
6.680345	407.339589	6.848998
6.420553	387.948037	6.854003
6.302347	386.465715	6.859008
5.776934	382.037453	6.864013
6.259311	372.493300	6.869018
6.215125	380.990079	6.874022
5.961662	383.342061	6.879027
6.110708	376.253871	6.884032
5.972933	386.517649	6.889037
6.180020	377.811387	6.894042
6.169772	378.048253	6.899046
6.057848	377.916474	6.904051
6.264310	375.913760	6.909056
6.036628	380.446403	6.914061
6.404121	362.092269	6.919066
5.660410	372.223149	6.924070
5.970270	379.166394	6.929075
6.533349	373.953493	6.934080
5.895164	378.297076	6.939085
6.202525	378.156976	6.944090
5.994309	388.684560	6.949094
5.806977	382.596288	6.954099
6.140564	377.888248	6.959104
6.209761	377.006155	6.964109
6.444003	374.794437	6.969114
6.393646	381.451128	6.974118
6.390259	376.727646	6.979123
6.275850	368.532577	6.984128
6.197982	382.662229	6.989133
6.309788	376.369142	6.994138
6.383453	375.751793	6.999142
6.248308	375.634605	7.004147
6.232589	363.379737	7.009152
6.048283	345.672735	7.014157
5.858824	347.602939	7.019162
5.900354	363.063728	7.024166
5.974917	382.186888	7.029171
5.952620	375.741737	7.034176
6.134728	382.821720	7.039181
5.966299	376.547320	7.044186
5.981960	379.730788	7.049190
5.965766	380.983012	7.054195
6.349926	377.340677	7.059200
5.741584	383.466374	7.064205
6.264844	381.674618	7.069210
6.081028	376.653614	7.074214
6.234021	371.577741	7.079219
6.599104	376.698966	7.084224
6.201639	372.476076	7.089229
6.023656	362.452184	7.094234
5.806917	365.752486	7.099238
6.077585	378.366014	7.104243
6.263750	371.946792	7.109248
6.048487	376.845465	7.114253
6.341426	378.095239	7.119258
6.173932	365.288317	7.124262
5.782395	368.710539	7.129267
6.171615	359.957713	7.134272
6.248374	372.876064	7.139277
6.162387	355.188220	7.144282
5.959797	357.190837	7.149286
5.860249	378.272562	7.154291
6.196825	379.267598	7.159296
5.734716	389.865850	7.164301
6.046149	373.963874	7.169306
6.188435	381.914659	7.174310
6.380031	384.211638	7.179315
6.449419	377.925856	7.184320
5.922757	362.921548	7.189325
6.098946	360.427603	7.194330
6.234838	375.188241	7.199334
5.733190	358.732627	7.204339
6.264527	367.402138	7.209344
5.685612	382.015626	7.214349
6.141503	379.349274	7.219354
6.030541	382.237181	7.224358
5.788786	392.427679	7.229363
5.858997	382.656358	7.234368
5.960703	381.434351	7.239373
5.808919	380.312443	7.244378
5.767717	378.853406	7.249382
5.796768	386.365244	7.254387
6.105167	392.645179	7.259392
6.287217	379.673340	7.264397
5.975576	370.741746	7.269402
6.085126	382.253483	7.274406
5.890570	385.832673	7.279411
6.534571	374.384986	7.284416
5.805438	389.923833	7.289421
6.081683	375.543218	7.294426
5.971209	385.364355	7.299430
5.973967	396.587326	7.304435
6.129929	371.987033	7.309440
5.736831	380.652066	7.314445
5.972080	383.628078	7.319450
6.214110	399.029428	7.324454
6.222356	400.017953	7.329459
6.416274	384.090598	7.334464
6.114119	380.609332	7.339469
6.068916	380.735265	7.344474
6.055662	384.247497	7.349478
6.013437	387.215203	7.354483
6.093580	371.986300	7.359488
5.603411	391.849880	7.364493
5.954362	405.592989	7.369498
6.366085	403.668325	7.374502
6.099655	406.803904	7.379507
6.091191	391.868426	7.384512
6.026374	403.489991	7.389517
6.451713	399.159332	7.394522
6.055387	392.252322	7.399526
6.033737	381.629394	7.404531
6.365878	381.031186	7.409536
6.374298	385.913713	7.414541
6.076797	368.667466	7.419546
5.731867	388.434034	7.424550
5.473250	388.366355	7.429555
6.232242	390.040576	7.434560
6.355296	415.620564	7.439565
6.005075	405.997534	7.444570
5.869744	396.891962	7.449574
6.320736	410.603448	7.454579
6.487332	403.779999	7.459584
6.331226	391.303150	7.464589
6.055956	384.813774	7.469594
6.056126	385.250471	7.474598
5.727795	388.819508	7.479603
6.144478	378.741431	7.484608
5.968137	393.405210	7.489613
6.230647	382.252994	7.494618
6.185832	384.029270	7.499622
6.264248	395.715554	7.504627
6.059636	379.362069	7.509632
5.855783	384.556897	7.514637
6.052344	374.854575	7.519642
6.130604	378.465925	7.524646
6.244098	391.034702	7.529651
6.509339	369.350370	7.534656
6.229161	382.445313	7.539661
6.259760	386.334858	7.544666
6.137537	377.510173	7.549670
6.132778	385.734365	7.554675
6.526335	382.241025	7.559680
6.311777	376.799896	7.564685
6.483079	386.186949	7.569690
6.660165	381.695571	7.574694
5.988847	362.066228	7.579699
5.884102	361.928330	7.584704
5.829740	364.743050	7.589709
6.014845	375.274387	7.594714
6.219326	381.068644	7.599718
6.021096	386.376294	7.604723
6.355660	382.745902	7.609728
6.334983	392.389422	7.614733
6.534491	363.835427	7.619738
6.381967	358.079998	7.624742
5.744097	360.668347	7.629747
6.049492	347.840314	7.634752
5.850757	357.751885	7.639757
5.998333	348.734746	7.644762
6.198524	351.755021	7.649766
5.844913	354.623928	7.654771
6.333074	346.544754	7.659776
5.909689	340.672693	7.664781
6.062117	344.446398	7.669786
5.933809	355.392765	7.674790
6.260750	366.829793	7.679795
6.125059	363.384062	7.684800
5.911696	348.779736	7.689805
6.215185	364.418027	7.694810
6.267163	363.728198	7.699814
5.586537	360.443458	7.704819
6.156276	364.320060	7.709824
6.150651	377.373968	7.714829
6.563872	376.058651	7.719834
6.125334	360.853423	7.724838
6.175092	363.208663	7.729843
6.355901	344.123486	7.734848
5.840573	349.673437	7.739853
5.924383	345.194229	7.744858
6.027994	345.241900	7.749862
5.836870	350.654318	7.754867
6.085704	349.031630	7.759872
6.371165	370.884836	7.764877
5.656927	365.452988	7.769882
6.007392	371.300166	7.774886
6.097877	376.209181	7.779891
6.239462	379.786981	7.784896
6.367133	389.738945	7.789901
6.122597	364.498082	7.794906
6.005364	357.065006	7.799910
5.790409	362.457394	7.804915
5.940984	369.038551	7.809920
5.978502	373.953360	7.814925
6.307088	379.060491	7.819930
6.347046	364.932228	7.824934
6.201995	373.750320	7.829939
6.042211	352.139507	7.834944
6.062243	375.554593	7.839949
6.235257	361.566238	7.844954
5.803949	360.025464	7.849958
5.718307	372.188217	7.854963
6.384352	367.304287	7.859968
5.898296	378.377271	7.864973
6.390142	383.579363	7.869978
6.267680	384.389414	7.874982
5.845897	375.770308	7.879987
6.173844	389.198547	7.884992
5.784133	374.508505	7.889997
5.878835	379.103199	7.895002
6.360959	386.566405	7.900006
6.063393	384.765470	7.905011
6.291028	380.094572	7.910016
5.853329	382.482031	7.915021
6.209785	379.251918	7.920026
6.399238	390.549397	7.925030
6.253254	379.681141	7.930035
6.308290	359.012000	7.935040
5.754904	365.637966	7.940045
5.910324	366.475790	7.945050
6.328988	372.259311	7.950054
6.274560	379.648698	7.955059
6.033763	354.816653	7.960064
6.262483	364.807050	7.965069
6.177110	362.174607	7.970074
5.947947	355.203289	7.975078
5.572158	359.384130	7.980083
5.873290	358.129662	7.985088
6.164127	370.876686	7.990093
6.312617	367.509580	7.995098
6.281856	376.765166	8.000102
6.146006	379.955519	8.005107
5.963717	371.342121	8.010112
6.144166	365.857031	8.015130
6.205014	372.579737	8.020147
6.084923	357.196821	8.025165
5.991102	370.255813	8.030182
6.403446	381.434019	8.035200
6.141135	362.451963	8.040218
6.086029	345.871471	8.045235
6.025757	350.511988	8.050253
6.181987	353.349791	8.055270
6.113241	345.955568	8.060288
6.039500	353.463038	8.065306
5.852015	365.570591	8.070323
6.045715	374.459448	8.075341
6.193737	380.806413	8.080358
6.763845	378.410214	8.085376
6.184576	375.351588	8.090394
5.888084	360.645022	8.095411
6.340474	370.780805	8.100429
6.207799	375.739723	8.105446
5.890601	360.195916	8.110464
6.158137	375.523623	8.115482
6.064385	380.823575	8.120499
6.293329	380.640375	8.125517
6.069194	385.454801	8.130534
6.265319	374.086642	8.135552
6.483481	392.791577	8.140570
6.099884	386.327424	8.145587
6.178197	395.289583	8.150605
6.110642	387.047394	8.155622
6.324281	379.757243	8.160640
6.133463	386.390766	8.165658
6.374423	389.048665	8.170675
6.337527	387.289768	8.175693
6.127854	393.471490	8.180710
6.360400	387.512273	8.185728
6.329816	392.453144	8.190746
6.171516	393.824956	8.195763
6.623116	380.921982	8.200781
6.289133	385.388006	8.205798
6.358736	388.094593	8.210816
6.640213	387.083991	8.215834
6.341836	366.621303	8.220851
6.008804	359.443743	8.225869
6.186401	378.380216	8.230886
6.225599	374.217238	8.235904
6.090245	381.323379	8.240922
6.031856	389.487339	8.245939
6.495914	381.626784	8.250957
6.082492	378.896675	8.255974
6.219370	378.847267	8.260992
6.405929	376.872447	8.266010
6.401983	385.460483	8.271027
6.229791	379.180641	8.276045
6.100696	389.875817	8.281062
6.401939	385.385734	8.286080
6.387551	385.240090	8.291098
6.325533	383.276828	8.296115
6.439890	384.186642	8.301133
6.235505	385.544715	8.306150
6.403275	389.076038	8.311168
6.449996	395.520047	8.316186
6.446087	396.717656	8.321203
6.332132	384.156120	8.326221
6.044505	395.560225	8.331238
6.250968	382.878627	8.336256
6.436903	394.604679	8.341274
5.884574	382.300097	8.346291
6.432583	395.527098	8.351309
6.421036	417.227160	8.356326
6.570138	418.430875	8.361344
6.560852	411.512025	8.366362
6.346678	408.886946	8.371379
6.464984	409.552756	8.376397
6.641164	416.605854	8.381414
6.538854	396.924033	8.386432
6.576108	394.430892	8.391450
6.190832	402.629298	8.396467
6.475596	394.087004	8.401485
6.447924	410.561917	8.406502
6.534443	420.802085	8.411520
6.683172	422.252364	8.416538
6.296125	408.897241	8.421555
6.674151	415.309829	8.426573
6.512261	424.351849	8.431590
6.235647	410.458606	8.436608
6.549386	413.821847	8.441626
6.459441	414.628742	8.446643
6.432660	416.678474	8.451661
6.677274	424.323877	8.456678
6.670096	422.503581	8.461696
6.514792	419.653463	8.466714
6.535816	417.515090	8.471731
6.544552	413.267391	8.476749
6.477591	428.041014	8.481766
6.571568	422.519259	8.486784
6.503059	408.386159	8.491802
6.468866	428.682409	8.496819
6.740804	412.466705	8.501837
6.712821	408.046079	8.506854
6.680842	418.609897	8.511872
6.975034	406.625832	8.516890
6.624853	418.731777	8.521907
6.726551	413.628345	8.526925
6.195632	420.864427	8.531942
6.275708	404.832177	8.536960
6.432446	410.089956	8.541978
6.404416	414.032596	8.546995
6.657522	404.984024	8.552013
6.302062	416.479062	8.557030
6.183679	415.729379	8.562048
6.539365	414.212819	8.567066
6.457415	415.343520	8.572083
7.035729	417.098611	8.577101
6.728813	412.442743	8.582119
6.450733	421.499141	8.587136
6.784986	426.947031	8.592154
6.618095	426.027056	8.597171
6.922017	431.510071	8.602189
6.868786	422.292082	8.607207
6.754101	418.170268	8.612224
7.080580	416.901395	8.617242
6.876295	420.977670	8.622259
6.669408	421.660813	8.627277
6.676123	414.097034	8.632295
6.560099	416.469616	8.637312
6.921962	415.801164	8.642330
6.456141	417.839118	8.647347
6.531953	414.007211	8.652365
6.342324	431.595292	8.657383
6.723644	441.946072	8.662400
7.035717	443.688680	8.667418
6.494887	452.544968	8.672435
6.779852	441.785468	8.677453
7.067691	457.605368	8.682471
6.713942	458.216149	8.687488
6.983929	451.016434	8.692506
6.664778	453.737879	8.697523
7.103932	454.910391	8.702541
6.970688	447.656082	8.707559
6.629745	448.636026	8.712576
6.887507	445.927438	8.717594
6.778611	452.168201	8.722611
7.026176	456.300396	8.727629
7.031038	453.456571	8.732647
6.733066	449.281395	8.737664
7.238710	445.382382	8.742682
6.484620	443.154135	8.747699
7.118201	431.966538	8.752717
6.822750	446.294479	8.757735
6.504894	455.663901	8.762752
6.839872	447.895102	8.767770
7.052887	448.567698	8.772787
6.998071	447.172211	8.777805
7.048904	457.909732	8.782823
6.799846	444.039457	8.787840
7.105391	453.121839	8.792858
6.884467	454.026744	8.797875
6.895562	445.884789	8.802893
6.800649	451.349391	8.807911
7.265564	444.424487	8.812928
7.067602	453.271347	8.817946
6.938847	457.710562	8.822963
6.929366	445.984875	8.827981
7.110042	456.112775	8.832999
6.819827	448.794366	8.838016
7.146573	452.861025	8.843034
6.984328	464.035449	8.848051
7.138400	446.548024	8.853069
6.978925	439.811625	8.858087
6.823821	443.674507	8.863104
6.996448	434.107934	8.868122
6.762404	450.426976	8.873139
7.028097	453.242378	8.878157
7.259443	439.215568	8.883175
7.086569	451.187632	8.888192
7.235840	440.655337	8.893210
7.194095	446.243307	8.898227
7.014794	442.758704	8.903245
6.832961	447.258744	8.908263
6.865687	444.609880	8.913280
7.129607	446.603604	8.918298
6.906943	460.349276	8.923315
6.838103	446.080299	8.928333
6.871698	451.364052	8.933351
6.940597	458.008217	8.938368
7.262325	452.138644	8.943386
6.894555	456.134390	8.948403
7.245173	448.267947	8.953421
7.121353	454.797829	8.958439
7.065960	453.320663	8.963456
7.195847	446.644587	8.968474
6.905812	447.662860	8.973491
6.928720	451.599552	8.978509
7.078933	445.698889	8.983527
6.693548	452.785273	8.988544
7.447661	447.764326	8.993562
7.073249	457.037999	8.998579
6.977938	455.133171	9.003597
7.183588	452.296511	9.008615
6.923277	461.534405	9.013632
7.460998	471.221698	9.018650
6.996816	478.427885	9.023667
7.047841	475.479302	9.028685
7.060321	481.503801	9.033703
7.249053	483.571162	9.038720
7.581412	480.092035	9.043738
7.597095	489.872696	9.048755
7.366851	468.862209	9.053773
7.450497	451.566300	9.058791
6.808380	458.901074	9.063808
7.249579	445.815945	9.068826
7.200374	448.994934	9.073843
6.938432	472.822822	9.078861
7.380094	471.153889	9.083879
7.057134	476.455736	9.088896
7.491540	470.155614	9.093914
7.267717	484.061603	9.098931
7.274151	484.896463	9.103949
7.432685	478.506130	9.108967
7.275592	473.901156	9.113984
7.482598	477.620265	9.119002
7.244865	490.598637	9.124019
7.287072	477.093399	9.129037
7.902840	479.187707	9.134055
7.324331	464.447349	9.139072
7.390216	447.913668	9.144090
7.438814	452.789221	9.149107
7.447432	446.168513	9.154125
7.564341	454.054674	9.159143
7.011021	450.898850	9.164160
7.138612	458.226968	9.169178
7.643285	476.529121	9.174195
7.534943	471.725384	9.179213
7.622666	445.702702	9.184231
7.119417	453.104564	9.189248
7.328044	461.063249	9.194266
7.563690	472.732436	9.199283
7.346372	478.376199	9.204301
7.761607	471.784916	9.209319
7.545231	461.652135	9.214336
7.533333	459.328883	9.219354
7.640675	447.587825	9.224371
6.941562	447.841792	9.229389
7.399994	453.610436	9.234407
7.542942	476.575524	9.239424
7.693907	465.071976	9.244442
7.344304	467.051468	9.249459
7.081658	457.504461	9.254477
7.363987	467.323013	9.259495
7.367006	476.520056	9.264512
7.384223	468.351690	9.269530
7.412250	475.055755	9.274547
7.278288	482.601777	9.279565
7.867687	479.045237	9.284583
7.458153	487.002473	9.289600
7.369746	479.737885	9.294618
7.513873	489.437194	9.299635
7.435129	485.389720	9.304653
7.323242	477.985539	9.309671
7.423199	479.984124	9.314688
7.935024	472.145741	9.319706
7.641082	485.779620	9.324723
7.251265	484.590345	9.329741
7.321544	477.982263	9.334759
7.122418	485.402175	9.339776
7.407473	492.684409	9.344794
7.554492	498.639742	9.349811
7.569864	514.313527	9.354829
7.718099	512.365787	9.359847
7.753134	513.555591	9.364864
7.696586	521.480391	9.369882
7.966385	516.481793	9.374899
7.549853	491.352631	9.379917
7.567025	482.613715	9.384935
7.314337	499.435588	9.389952
7.587905	498.292357	9.394970
8.200555	511.490177	9.399987
7.566777	507.780138	9.405005
8.024318	502.464359	9.410023
7.553026	492.058790	9.415040
7.468979	491.901630	9.420058
7.703912	498.910713	9.425075
7.660781	513.932396	9.430093
8.066354	523.576712	9.435111
7.915806	506.503067	9.440128
7.598163	492.266899	9.445146
7.786097	495.544868	9.450163
7.627768	509.076451	9.455181
8.111812	499.322771	9.460199
7.937146	493.279954	9.465216
7.467754	487.011002	9.470234
7.827686	477.790534	9.475251
7.627902	491.627905	9.480269
8.008458	500.270351	9.485287
7.705473	498.905145	9.490304
7.944027	483.525812	9.495322
7.545395	487.082763	9.500339
7.485082	499.756191	9.505357
7.777863	501.074328	9.510375
7.653260	509.107690	9.515392
7.910455	511.088462	9.520410
8.323225	507.914575	9.525427
7.820467	521.266229	9.530445
8.010531	506.010315	9.535463
7.990202	505.617672	9.540480
7.844912	514.063228	9.545498
7.771432	511.926388	9.550515
7.823268	519.867421	9.555533
7.829723	505.363650	9.560551
7.608127	521.954374	9.565568
7.705103	523.367555	9.570586
7.954547	509.028109	9.575603
7.958058	513.653214	9.580621
8.100396	512.669929	9.585639
8.386578	510.593311	9.590656
7.890719	522.101592	9.595674
7.870641	516.547187	9.600691
7.933141	523.637818	9.605709
8.604939	511.318689	9.610727
7.976787	510.562319	9.615744
7.968855	494.258065	9.620762
7.996515	496.415813	9.625779
7.854841	507.991804	9.630797
8.220403	496.939379	9.635815
8.036353	505.432862	9.640832
7.609281	510.305072	9.645850
8.007199	507.309685	9.650867
8.023165	516.663142	9.655885
8.231889	509.808002	9.660903
7.849122	512.923748	9.665920
7.663219	517.847620	9.670938
7.985391	510.350633	9.675955
7.505256	510.792677	9.680973
8.020868	509.016263	9.685991
7.961149	517.599714	9.691008
7.659742	511.292658	9.696026
7.926260	509.988717	9.701043
7.627183	528.214255	9.706061
7.911489	529.617046	9.711079
8.057189	554.153910	9.716096
8.113011	552.867072	9.721114
8.184793	542.386088	9.726131
8.029618	557.835694	9.731149
8.273890	552.291023	9.736167
8.126207	552.561911	9.741184
8.083991	551.846376	9.746202
8.642716	546.934541	9.751219
8.066370	544.539728	9.756237
8.369713	541.337964	9.761255
8.483325	548.798329	9.766272
8.336530	525.719771	9.771290
8.462583	517.838840	9.776307
8.036854	518.760177	9.781325
7.924295	501.211067	9.786343
8.026636	503.425358	9.791360
8.180385	524.059102	9.796378
8.231786	534.572711	9.801395
8.301402	543.639424	9.806413
8.486243	538.848225	9.811431
8.340920	532.353293	9.816448
7.886748	530.448718	9.821466
8.365007	538.390733	9.826483
8.177749	544.090071	9.831501
8.220606	548.415732	9.836519
8.381658	551.287710	9.841536
8.297041	540.831294	9.846554
8.437892	536.998251	9.851571
8.125236	549.646704	9.856589
8.501419	539.084321	9.861607
8.664476	537.960729	9.866624
8.317050	524.840639	9.871642
8.625108	518.321467	9.876659
7.962019	519.475198	9.881677
7.957544	525.357959	9.886695
8.217266	535.628426	9.891712
8.495202	531.695975	9.896730
8.533283	553.144180	9.901747
8.547495	546.020444	9.906765
8.518722	539.287396	9.911783
8.356341	550.029219	9.916800
8.382738	549.636233	9.921818
8.806241	537.856734	9.926835
8.362160	538.200024	9.931853
8.488621	529.700545	9.936871
8.366531	536.797382	9.941888
8.166187	543.191553	9.946906
8.797349	536.953849	9.951923
8.213007	546.353785	9.956941
8.331633	545.581559	9.961959
8.455997	550.145274	9.966976
8.403440	554.893315	9.971994
8.458410	542.780013	9.977011
8.203380	557.089567	9.982029
8.416078	549.953889	9.987047
8.315037	551.626719	9.992064
8.529521	552.627554	9.997082
8.523659	548.812259	10.002099
8.439577	549.982685	10.007117
8.606533	534.341666	10.012135
8.783827	546.725721	10.017152
8.388141	548.366551	10.022170
8.516914	549.121466	10.027187
8.315145	553.847029	10.032205
8.359250	543.207561	10.037223
8.627717	546.606260	10.042240
8.357867	554.987205	10.047258
8.613548	545.869536	10.052275
8.462955	549.910698	10.057293
8.540383	551.923348	10.062311
8.743335	550.626562	10.067328
8.732806	550.692735	10.072346
8.881826	552.342150	10.077363
8.828718	547.082798	10.082381
8.563658	549.480522	10.087399
8.524451	547.077240	10.092416
7.963877	555.227842	10.097434
8.390378	549.745755	10.102451
8.319348	575.788147	10.107469
8.628104	581.285179	10.112487
8.986166	578.091289	10.117504
9.037343	581.291111	10.122522
9.114853	579.353771	10.127539
8.816404	569.199252	10.132557
8.623506	557.931657	10.137575
8.862506	543.154232	10.142592
8.809998	542.406645	10.147610
8.904686	543.781534	10.152627
8.594949	554.875105	10.157645
8.490116	546.347811	10.162663
8.993337	554.420327	10.167680
8.783831	567.040825	10.172698
8.744465	553.397358	10.177715
8.941126	564.184067	10.182733
8.744378	551.733694	10.187751
8.770421	549.645546	10.192768
8.509671	565.604631	10.197786
8.881715	575.347514	10.202803
9.170511	564.529236	10.207821
9.050160	574.092816	10.212839
9.197232	555.413558	10.217856
9.093796	541.261900	10.222874
8.731951	552.856794	10.227891
8.640258	546.424534	10.232909
8.624983	536.461085	10.237927
8.625282	558.071218	10.242944
8.806623	569.108541	10.247962
8.745772	569.521051	10.252979
8.691266	576.584596	10.257997
8.603174	574.902530	10.263015
8.940505	574.736153	10.268032
8.725526	576.195776	10.273050
8.864707	576.806875	10.278067
8.829250	578.608212	10.283085
8.996082	582.288326	10.288103
9.063389	582.415931	10.293120
8.922243	592.553413	10.298138
8.835331	576.645412	10.303155
8.910214	589.530677	10.308173
9.194590	587.004538	10.313191
8.894558	572.549385	10.318208
9.008226	585.985998	10.323226
9.277215	579.347101	10.328243
9.089208	581.398208	10.333261
9.052291	593.702469	10.338279
9.180578	566.811735	10.343296
8.854783	583.100223	10.348314
9.078559	586.287464	10.353331
9.260869	572.577136	10.358349
9.111564	582.639794	10.363367
9.328039	575.203049	10.368384
9.069885	580.850252	10.373402
9.193764	576.902706	10.378419
9.192071	577.293237	10.383437
9.013274	580.378634	10.388455
9.272288	579.287006	10.393472
8.930825	590.932191	10.398490
8.923027	576.975479	10.403507
9.182298	580.915556	10.408525
9.185944	585.336076	10.413543
8.939992	578.554962	10.418560
8.467270	580.197210	10.423578
9.019828	590.691017	10.428595
9.521487	593.159048	10.433613
9.273874	601.011843	10.438631
9.374684	589.602299	10.443648
9.314130	578.404236	10.448666
9.326004	576.735663	10.453683
9.290043	579.619243	10.458701
8.980174	571.459413	10.463719
9.060019	575.551260	10.468736
9.126934	592.855151	10.473754
9.284588	599.281110	10.478771
9.635161	599.781602	10.483789
9.361163	601.370739	10.488807
9.446468	574.867529	10.493824
9.317345	567.743459	10.498842
9.207176	579.419591	10.503859
9.082210	573.332512	10.508877
8.771335	589.977524	10.513895
9.548975	596.201044	10.518912
9.486270	605.481944	10.523930
9.616014	603.491489	10.528947
9.582079	601.072370	10.533965
9.314491	594.542904	10.538983
9.481045	586.847037	10.544000
9.162416	582.392125	10.549018
9.109602	590.400479	10.554035
9.428719	586.897439	10.559053
9.623176	602.619558	10.564071
9.648101	601.586491	10.569088
9.695968	602.149013	10.574106
9.412510	586.818647	10.579123
9.374693	582.945842	10.584141
9.071280	582.862918	10.589159
9.472829	593.186446	10.594176
9.820049	604.509212	10.599194
9.500907	597.003425	10.604211
9.531944	601.380160	10.609229
9.524863	599.730461	10.614247
9.252962	574.543114	10.619264
9.623683	599.367306	10.624282
9.819789	608.126695	10.629299
9.456161	573.308531	10.634317
9.353787	593.583793	10.639335
9.297819	591.062826	10.644352
9.329636	603.506296	10.649370
9.220487	607.895571	10.654387
9.492349	611.255739	10.659405
9.534074	604.221406	10.664423
9.705168	604.316115	10.669440
9.510231	603.472304	10.674458
9.556406	603.727196	10.679475
9.670083	595.465967	10.684493
9.449393	612.275393	10.689511
9.660603	602.292677	10.694528
9.496333	612.067828	10.699546
9.660517	614.659139	10.704563
9.661760	597.208215	10.709581
9.542213	607.785256	10.714599
9.657974	606.571168	10.719616
9.463430	606.726401	10.724634
9.358320	603.401906	10.729651
9.849802	605.982918	10.734669
9.779146	593.187821	10.739687
9.865695	595.095349	10.744704
9.568999	608.431919	10.749722
9.545582	606.340915	10.754739
9.955180	606.704907	10.759757
9.570279	603.481166	10.764775
9.960216	609.077171	10.769792
9.937793	616.641826	10.774810
9.854178	607.536993	10.779827
9.925376	603.681987	10.784845
9.469390	614.724982	10.789863
9.814016	598.404865	10.794880
9.632373	601.973611	10.799898
9.805584	603.644619	10.804915
9.771741	606.189143	10.809933
9.739586	612.872316	10.814951
10.012961	625.102592	10.819968
10.027262	612.104010	10.824986
10.178605	610.871543	10.830003
9.491821	594.981570	10.835021
9.424158	616.877469	10.840039
9.746171	638.645924	10.845056
10.071615	636.722514	10.850074
9.862835	636.121786	10.855091
9.997470	644.260478	10.860109
9.924032	638.231479	10.865127
10.208067	633.355270	10.870144
9.743430	641.239128	10.875162
9.832051	644.791069	10.880179
10.127292	630.268288	10.885197
9.866129	648.764321	10.890215
9.975811	641.771289	10.895232
9.926731	633.916289	10.900250
9.776995	644.312259	10.905267
10.271118	636.834718	10.910285
10.369882	639.050899	10.915303
10.410463	636.301905	10.920320
10.014975	608.616435	10.925338
9.715642	608.409633	10.930355
10.270537	619.194747	10.935373
10.254571	637.385437	10.940391
10.236488	626.892972	10.945408
10.368601	616.209683	10.950426
9.745651	608.201355	10.955443
10.229987	601.202222	10.960461
10.047841	611.272491	10.965479
10.104336	596.848633	10.970496
10.101490	603.452760	10.975514
9.768645	610.967945	10.980531
10.229276	625.535203	10.985549
10.129056	633.934801	10.990567
10.297859	629.209499	10.995584
10.279268	634.476354	11.000602
10.346527	635.634175	11.005619
10.534293	618.441714	11.010637
10.141663	613.214437	11.015655
10.407937	614.837691	11.020672
10.376066	608.971190	11.025690
10.064992	611.882725	11.030707
10.284010	605.698245	11.035725
9.876040	609.044113	11.040743
9.652382	622.697101	11.045760
10.190798	631.661102	11.050778
10.219143	633.420608	11.055795
10.287905	636.127279	11.060813
10.022178	642.085536	11.065831
10.087295	635.326105	11.070848
10.186121	638.085966	11.075866
10.046818	634.905670	11.080883
10.154746	630.251735	11.085901
10.152885	650.032702	11.090919
10.148752	642.002291	11.095936
10.302052	640.994750	11.100954
10.261602	642.706484	11.105971
10.240334	639.591113	11.110989
10.308407	647.169562	11.116007
10.332542	666.787625	11.121024
10.328707	660.857132	11.126042
10.252108	670.460087	11.131059
10.594958	679.477100	11.136077
10.441647	677.109973	11.141095
10.520567	662.513779	11.146112
10.922941	670.955315	11.151130
10.478207	656.015436	11.156147
10.590453	634.614822	11.161165
10.410731	644.519883	11.166183
10.526359	639.681343	11.171200
10.450107	634.407286	11.176218
10.094730	646.722789	11.181235
10.227466	646.895083	11.186253
10.467100	651.571643	11.191271
10.552213	669.686820	11.196288
10.451108	669.858987	11.201306
10.165813	670.065923	11.206323
10.466196	674.861952	11.211341
10.232123	666.661401	11.216359
10.397175	677.506552	11.221376
10.560493	666.423071	11.226394
10.273678	676.267815	11.231411
10.509243	665.741377	11.236429
10.502837	682.521864	11.241447
10.309597	677.511466	11.246464
10.677396	683.487067	11.251482
10.788242	707.259418	11.256499
10.895833	698.333817	11.261517
10.682210	681.791165	11.266535
10.324592	689.208631	11.271552
10.879527	689.732331	11.276570
10.748098	689.928305	11.281587
10.815209	677.596791	11.286605
10.906707	674.557641	11.291623
10.514175	675.238901	11.296640
10.673559	670.116994	11.301658
10.443713	686.126401	11.306675
10.795206	697.993698	11.311693
11.073746	703.038081	11.316711
10.951784	695.587635	11.321728
10.794147	680.321109	11.326746
10.501524	680.150296	11.331763
10.690338	696.769231	11.336781
11.012444	701.180553	11.341799
11.096702	711.980628	11.346816
10.666058	690.681069	11.351834
10.835336	697.994245	11.356851
10.900899	698.852016	11.361869
10.877976	690.908035	11.366887
10.933965	707.547751	11.371904
10.900322	691.930178	11.376922
10.760196	698.606432	11.381939
11.044361	701.187673	11.386957
10.923033	696.282586	11.391975
10.719108	711.606571	11.396992
11.175722	711.534730	11.402010
11.194972	701.880466	11.407027
11.054298	680.684644	11.412045
10.930594	677.148485	11.417063
10.328951	673.845315	11.422080
11.192405	675.390356	11.427098
11.192450	696.428692	11.432115
10.829290	702.993411	11.437133
11.014876	702.817964	11.442151
10.990821	700.098928	11.447168
11.177551	704.249706	11.452186
11.000232	715.296514	11.457203
10.844487	702.904092	11.462221
10.845307	711.288708	11.467239
11.269043	711.601163	11.472256
11.340511	696.815851	11.477274
11.181646	711.155120	11.482291
11.046783	711.132512	11.487309
11.151423	706.039026	11.492327
11.074233	704.100764	11.497344
10.789423	701.338125	11.502362
10.869678	702.578137	11.507379
10.758646	703.441770	11.512397
10.921929	697.833478	11.517415
10.944781	705.044896	11.522432
11.066808	692.423247	11.527450
10.559629	706.720881	11.532467
11.068038	705.666164	11.537485
11.397210	712.447215	11.542503
11.306604	701.815336	11.547520
11.072313	707.656339	11.552538
11.278340	713.184762	11.557555
11.416916	711.208087	11.562573
11.369506	708.475984	11.567591
11.302505	712.147045	11.572608
11.353885	702.603098	11.577626
11.206637	711.778667	11.582643
10.999599	704.391675	11.587661
11.223106	712.456180	11.592679
11.238876	733.268587	11.597696
11.115958	719.611227	11.602714
10.818067	734.436395	11.607731
10.936457	729.878123	11.612749
11.040017	725.783926	11.617767
10.940810	736.155863	11.622784
11.202759	735.404913	11.627802
11.215504	742.304399	11.632819
11.556875	755.795540	11.637837
11.754083	763.525802	11.642855
11.303642	731.717310	11.647872
11.455562	734.396577	11.652890
11.428460	736.293087	11.657907
11.509710	732.198836	11.662925
11.537248	731.035138	11.667943
11.490025	737.586530	11.672960
11.460404	725.760927	11.677978
11.532481	727.591843	11.682995
11.663874	731.714183	11.688013
11.726494	731.928965	11.693031
11.342009	724.560857	11.698048
11.285659	731.229481	11.703066
11.694846	740.512482	11.708083
11.473424	746.308566	11.713101
11.787129	770.147865	11.718119
11.591040	749.998308	11.723136
11.834061	725.625542	11.728154
11.469170	732.898296	11.733171
11.376826	738.931263	11.738189
11.606878	734.526944	11.743207
11.444529	761.479745	11.748224
11.642949	762.589134	11.753242
11.734513	754.667531	11.758259
11.627204	762.645421	11.763277
11.542885	759.388998	11.768295
11.587258	758.229994	11.773312
11.519569	758.796661	11.778330
11.543369	755.005050	11.783347
11.659649	757.789700	11.788365
11.698550	742.598584	11.793383
11.580608	755.524318	11.798400
11.667047	746.119994	11.803418
11.563993	755.622374	11.808435
11.815659	757.696889	11.813453
11.752487	754.610266	11.818471
11.753870	760.227338	11.823488
11.961607	750.727783	11.828506
11.817092	757.356570	11.833523
11.753940	755.513207	11.838541
11.900226	755.569014	11.843559
11.741293	746.730433	11.848576
11.979019	760.039729	11.853594
11.758878	753.370392	11.858611
11.651910	752.538703	11.863629
11.920464	763.149037	11.868647
11.933791	759.917415	11.873664
11.702277	753.258911	11.878682
11.635115	766.102753	11.883699
11.979225	770.981923	11.888717
12.057092	764.679493	11.893735
11.784238	782.386727	11.898752
11.964352	779.343342	11.903770
11.793591	790.657376	11.908787
11.782638	791.365820	11.913805
12.338144	786.248282	11.918823
12.313663	796.611059	11.923840
12.372331	796.116394	11.928858
11.944271	763.560677	11.933875
11.761074	774.901749	11.938893
12.123115	776.850961	11.943911
12.096622	780.376395	11.948928
12.050951	789.678306	11.953946
11.749193	789.631714	11.958963
12.047110	788.918313	11.963981
12.152290	793.215047	11.968999
12.028935	806.369726	11.974016
12.075309	792.611109	11.979034
11.754242	795.031510	11.984051
11.620425	790.872508	11.989069
11.873057	793.715718	11.994087
11.809727	795.332155	11.999104
11.778910	793.928931	12.004122
12.076479	810.963694	12.009139
12.411659	818.850677	12.014157
12.727637	829.363473	12.019175
12.118440	811.345103	12.024192
11.834717	791.944382	12.029210
12.476912	811.745475	12.034227
12.366143	830.385541	12.039245
12.340729	822.071600	12.044263
12.118288	807.723458	12.049280
12.261397	833.003575	12.054298
12.070459	824.182539	12.059315
12.525244	835.497049	12.064333
12.556636	830.089015	12.069351
12.432667	840.665569	12.074368
12.506350	833.367040	12.079386
12.432794	800.726679	12.084403
12.381971	801.252379	12.089421
12.359041	805.120078	12.094439
12.488466	804.572094	12.099456
12.838811	814.995555	12.104474
12.532235	810.127246	12.109491
12.280325	794.506276	12.114509
12.553877	794.355555	12.119527
12.384128	804.455588	12.124544
12.034002	797.326996	12.129562
12.651486	800.355142	12.134579
12.565137	815.800521	12.139597
12.574478	787.355734	12.144615
12.350759	798.862447	12.149632
12.539090	805.373662	12.154650
12.506318	820.006800	12.159667
12.344199	824.285720	12.164685
12.658305	826.152719	12.169703
12.438981	836.741486	12.174720
12.866066	829.434153	12.179738
12.799681	822.604657	12.184755
12.368339	827.548720	12.189773
12.580154	823.353256	12.194791
12.635099	829.456979	12.199808
12.608443	834.184982	12.204826
12.751887	828.023137	12.209843
12.613373	829.065892	12.214861
12.528045	832.758314	12.219879
12.766537	823.223619	12.224896
12.691077	821.851288	12.229914
12.911077	821.201049	12.234931
12.902540	832.599504	12.239949
12.871558	814.861981	12.244967
12.533550	824.771666	12.249984
12.547923	834.944127	12.255002
12.786444	832.380751	12.260019
12.470469	825.170631	12.265037
12.743661	823.334658	12.270055
12.802027	828.719938	12.275072
12.642358	832.793967	12.280090
13.127068	822.688859	12.285107
12.738208	829.599742	12.290125
12.916352	826.033249	12.295143
12.671744	825.817202	12.300160
12.753298	822.858391	12.305178
12.445399	829.561739	12.310195
12.414738	821.863215	12.315213
12.832812	825.020561	12.320231
12.932565	835.306349	12.325248
12.607925	833.571237	12.330266
12.948752	851.400419	12.335283
13.108497	859.447788	12.340301
13.213540	852.470975	12.345319
13.093174	842.280252	12.350336
12.924873	831.049328	12.355354
13.103256	821.381090	12.360371
12.705933	839.519807	12.365389
12.863103	839.987420	12.370407
13.216067	842.936083	12.375424
12.954129	853.669378	12.380442
13.123169	856.882056	12.385459
12.945468	858.299724	12.390477
12.910070	854.587642	12.395495
13.208087	862.017981	12.400512
13.069323	862.482639	12.405530
13.223590	861.926218	12.410547
13.223715	869.131726	12.415565
13.336745	863.447246	12.420583
13.409893	864.294621	12.425600
13.177735	871.046876	12.430618
13.201585	851.234097	12.435635
13.083382	853.710827	12.440653
13.205994	862.210511	12.445671
13.297396	862.189381	12.450688
13.155670	851.514379	12.455706
13.217103	861.500570	12.460723
12.997428	865.284481	12.465741
13.598053	849.214160	12.470759
13.405075	860.065369	12.475776
12.851959	874.750600	12.480794
13.237370	852.136648	12.485811
12.811283	865.061831	12.490829
13.034173	867.367748	12.495847
13.331777	858.522148	12.500864
13.319892	866.701506	12.505882
13.647369	864.259424	12.510899
13.282932	855.529629	12.515917
13.376034	863.455853	12.520935
13.154860	870.148626	12.525952
13.283392	858.198182	12.530970
13.572907	861.289888	12.535987
13.008131	865.896041	12.541005
13.365002	860.055441	12.546023
13.321791	878.386916	12.551040
13.409793	885.111756	12.556058
13.841916	885.483645	12.561075
13.592599	891.444403	12.566093
13.426190	899.989017	12.571111
13.584689	894.297798	12.576128
13.735850	893.665427	12.581146
13.659474	871.995513	12.586163
13.423735	876.197949	12.591181
13.608221	878.969578	12.596199
13.872263	878.561815	12.601216
13.695249	859.802503	12.606234
13.894717	857.096491	12.611251
13.348890	850.529644	12.616269
13.378391	855.641017	12.621287
13.694128	863.012041	12.626304
13.904273	873.468060	12.631322
13.745832	860.373527	12.636339
13.659073	866.871775	12.641357
13.769477	856.556407	12.646375
13.476099	856.882571	12.651392
13.445236	877.234758	12.656410
13.751466	874.135579	12.661427
13.606753	891.903735	12.666445
13.620052	885.206981	12.671463
13.954195	884.465153	12.676480
13.458254	892.565887	12.681498
13.937598	889.319220	12.686515
13.799029	884.384940	12.691533
13.755427	887.362540	12.696551
13.888701	881.940899	12.701568
13.893514	891.608869	12.706586
13.593285	897.851221	12.711603
13.578271	901.843499	12.716621
13.639172	887.442062	12.721639
13.884828	874.708807	12.726656
13.603500	887.711348	12.731674
13.843885	889.981312	12.736691
13.721070	912.202534	12.741709
14.110930	925.583861	12.746727
13.797707	923.130447	12.751744
14.111146	928.245207	12.756762
14.427181	917.309308	12.761779
13.782956	907.706794	12.766797
14.008562	911.000966	12.771815
14.393273	914.007180	12.776832
13.841104	906.205757	12.781850
13.945848	908.292567	12.786867
14.100976	913.769741	12.791885
13.836070	929.953963	12.796903
14.169695	903.209482	12.801920
13.766391	914.779517	12.806938
13.952088	913.482994	12.811955
14.070197	921.790380	12.816973
14.046637	926.611681	12.821991
14.236145	913.484499	12.827008
13.801044	924.756997	12.832026
14.165754	919.159325	12.837043
14.233013	920.319530	12.842061
13.866205	929.531905	12.847079
14.162538	915.598234	12.852096
13.935680	914.637164	12.857114
14.276813	913.190272	12.862131
13.953363	923.041818	12.867149
14.101073	941.352937	12.872167
14.264301	952.096437	12.877184
14.625838	954.816778	12.882202
14.637266	949.680161	12.887219
14.427698	952.817461	12.892237
14.191386	940.984420	12.897255
14.439259	940.202132	12.902272
14.401628	950.714896	12.907290
14.847264	943.693467	12.912307
14.344603	931.674373	12.917325
14.340585	923.470502	12.922343
14.434216	909.867229	12.927360
14.179047	920.865938	12.932378
14.476108	932.299580	12.937395
15.114675	939.115019	12.942413
14.511202	923.892604	12.947431
15.082700	923.258570	12.952448
14.283033	920.510318	12.957466
14.771954	914.237418	12.962483
14.385494	921.971221	12.967501
14.283697	918.725131	12.972519
14.541130	913.024445	12.977536
14.528208	912.569850	12.982554
14.400371	913.379097	12.987571
14.613593	934.481232	12.992589
14.433818	942.228026	12.997607
14.715149	951.663462	13.002624
14.459054	959.920032	13.007642
14.857433	940.624668	13.012659
14.977696	949.176451	13.017677
14.956461	953.345231	13.022695
15.333216	929.820752	13.027712
14.734857	918.010854	13.032730
14.953093	919.079290	13.037747
14.517575	916.311207	13.042765
14.285272	920.728402	13.047783
14.467539	913.788298	13.052800
14.877864	939.857251	13.057818
14.852881	940.774677	13.062835
14.289141	941.890663	13.067853
14.742771	947.949607	13.072871
15.136705	951.653784	13.077888
14.686460	953.977468	13.082906
14.774292	942.464217	13.087923
14.937519	949.701854	13.092941
14.771170	949.544218	13.097959
14.994332	933.263599	13.102976
14.948719	953.957535	13.107994
14.484971	950.589692	13.113011
15.029467	943.669326	13.118029
14.835695	948.704064	13.123047
15.090767	947.857211	13.128064
14.772517	950.147863	13.133082
14.997999	952.356630	13.138099
14.998885	949.159596	13.143117
14.764354	955.356967	13.148135
14.996155	950.861369	13.153152
14.787393	944.804130	13.158170
14.735963	959.642416	13.163187
15.019562	958.627099	13.168205
14.793878	979.484563	13.173223
15.073070	980.361662	13.178240
15.115549	978.247023	13.183258
15.206052	985.011644	13.188275
15.351473	982.553377	13.193293
15.012705	976.066509	13.198311
15.198492	981.334248	13.203328
15.184583	985.246261	13.208346
15.132354	979.927571	13.213363
15.471238	975.832404	13.218381
15.153975	978.539653	13.223399
15.323550	970.419352	13.228416
15.407433	982.110661	13.233434
15.345354	985.019791	13.238451
15.183092	979.305382	13.243469
14.836646	980.943925	13.248487
15.176931	978.235089	13.253504
15.008842	981.987476	13.258522
15.093644	988.140944	13.263539
15.109316	979.761477	13.268557
15.348939	992.118272	13.273575
15.471897	1000.733800	13.278592
15.326459	1007.481329	13.283610
15.433269	1006.440018	13.288627
15.636147	999.206265	13.293645
15.377280	1017.400543	13.298663
15.861446	1003.986246	13.303680
15.751535	996.448145	13.308698
15.319426	992.976755	13.313715
15.665179	987.405416	13.318733
15.380563	981.466880	13.323751
15.468672	983.885623	13.328768
15.369371	991.526541	13.333786
15.288123	1022.521287	13.338803
15.570041	1016.080524	13.343821
15.443873	1009.575434	13.348839
15.754685	1011.339869	13.353856
15.599142	1017.131859	13.358874
15.596237	1024.144570	13.363891
15.953515	1010.997255	13.368909
15.569590	1014.566557	13.373927
15.826749	1011.516791	13.378944
15.814020	1019.380875	13.383962
15.636185	1007.921516	13.388979
15.714038	1023.008431	13.393997
15.561315	1013.047608	13.399015
15.937492	1009.853589	13.404032
15.654489	1023.476687	13.409050
15.206629	1013.892729	13.414067
15.809159	1008.022596	13.419085
15.423563	1021.777981	13.424103
15.361658	1018.681845	13.429120
16.007848	1025.752515	13.434138
16.156504	1033.065519	13.439155
16.160114	1009.475145	13.444173
15.782832	1017.010269	13.449191
15.644770	1015.132609	13.454208
16.130229	1022.403136	13.459226
15.858869	1017.427974	13.464243
15.959180	1018.899203	13.469261
16.223568	1037.744405	13.474279
15.696586	1021.430601	13.479296
15.914027	1028.808404	13.484314
16.102247	1034.217467	13.489331
16.298058	1038.013452	13.494349
16.125814	1042.001538	13.499367
16.220468	1009.309024	13.504384
16.263657	1006.756644	13.509402
16.045627	997.517423	13.514419
16.192633	999.356655	13.519437
16.214406	1010.117471	13.524455
16.155980	1000.474380	13.529472
16.148894	993.092092	13.534490
15.828077	997.992949	13.539507
16.249442	1009.251900	13.544525
16.265852	1018.571737	13.549543
16.446931	1026.190152	13.554560
16.298105	1000.436390	13.559578
16.131668	999.453520	13.564595
16.291017	998.218323	13.569613
16.292365	1011.861337	13.574631
16.531540	1005.763999	13.579648
16.535613	1006.030973	13.584666
16.134416	1010.253998	13.589683
16.292646	1000.827322	13.594701
16.144888	1007.899981	13.599719
16.308172	1020.474692	13.604736
16.728723	1028.186975	13.609754
16.276530	1028.989998	13.614771
16.635127	1027.241346	13.619789
16.424381	1028.014112	13.624807
16.099390	1018.189215	13.629824
16.762383	1027.550210	13.634842
16.263531	1032.395277	13.639859
16.803057	1025.360362	13.644877
16.488019	1036.172428	13.649895
16.743932	1038.201111	13.654912
16.367208	1016.824680	13.659930
16.316592	1029.472044	13.664947
16.523872	1037.258447	13.669965
16.538017	1032.787970	13.674983
16.247590	1039.479074	13.680000
16.624170	1035.996845	13.685018
16.336761	1040.666643	13.690035
16.510606	1035.646439	13.695053
16.238233	1042.092280	13.700071
16.246558	1026.986041	13.705088
16.329222	1042.119514	13.710106
16.358820	1061.435458	13.715123
16.678281	1053.604955	13.720141
16.141157	1064.136376	13.725159
16.637456	1069.016668	13.730176
16.827273	1062.441624	13.735194
16.691379	1066.525267	13.740211
16.878661	1067.617329	13.745229
16.857603	1073.749356	13.750247
16.833829	1064.223804	13.755264
16.769704	1072.783297	13.760282
16.881120	1073.055954	13.765299
17.228458	1063.492888	13.770317
17.118133	1063.597993	13.775335
16.964803	1067.310369	13.780352
17.255514	1065.091124	13.785370
16.975136	1068.036444	13.790387
17.058006	1058.621694	13.795405
17.453975	1058.293387	13.800423
17.042006	1059.700387	13.805440
17.337734	1065.506681	13.810458
17.244426	1069.168398	13.815475
17.252147	1072.199943	13.820493
17.298460	1055.028403	13.825511
16.834814	1045.436012	13.830528
17.045492	1049.987581	13.835546
17.383453	1053.676038	13.840563
17.200731	1038.775739	13.845581
17.302973	1029.986829	13.850599
17.069812	1030.277164	13.855616
17.517475	1031.356307	13.860634
16.826308	1024.930902	13.865651
17.185351	1019.318386	13.870669
17.257241	1026.540057	13.875687
17.295706	1042.306807	13.880704
17.528123	1026.040799	13.885722
17.214740	1028.922483	13.890739
17.216317	1021.169622	13.895757
16.873552	1032.213886	13.900775
16.780761	1044.978646	13.905792
17.134202	1047.217945	13.910810
17.048980	1056.486600	13.915827
17.002584	1056.680729	13.920845
17.371212	1061.422696	13.925863
17.448223	1054.825753	13.930880
17.514276	1045.695533	13.935898
17.574833	1051.591563	13.940915
17.441842	1054.783441	13.945933
17.608022	1047.984789	13.950951
17.396827	1054.219280	13.955968
17.267580	1059.712602	13.960986
17.430289	1065.188381	13.966003
17.734045	1059.151302	13.971021
17.622396	1060.624597	13.976039
17.686748	1062.363834	13.981056
17.608582	1054.245657	13.986074
17.336688	1061.555647	13.991091
17.521323	1057.729608	13.996109
17.501290	1058.483062	14.001127
17.298544	1056.061163	14.006144
17.741487	1058.232729	14.011162
17.385904	1087.421097	14.016179
17.426328	1092.247327	14.021197
17.930013	1088.814345	14.026215
17.357251	1094.335311	14.031232
18.116132	1082.798938	14.036250
18.253630	1091.712162	14.041267
17.967957	1088.326571	14.046285
18.174956	1075.491388	14.051303
17.887877	1085.078901	14.056320
17.651675	1070.840840	14.061338
18.148153	1078.965528	14.066355
17.838135	1071.005814	14.071373
17.832906	1069.100291	14.076391
17.764985	1072.567492	14.081408
17.915639	1084.509709	14.086426
17.944410	1087.538369	14.091443
17.896035	1084.032671	14.096461
18.012907	1085.926885	14.101479
17.672811	1091.011043	14.106496
17.899385	1078.813556	14.111514
17.705534	1094.807106	14.116531
18.036922	1089.960127	14.121549
18.153004	1083.164818	14.126567
17.928454	1102.298148	14.131584
18.142778	1091.440833	14.136602
18.098889	1092.618828	14.141619
18.382007	1090.746248	14.146637
18.186853	1094.999507	14.151655
17.916825	1098.524321	14.156672
18.488378	1096.868990	14.161690
17.968160	1091.344380	14.166707
17.932685	1083.282410	14.171725
17.929976	1078.834583	14.176743
17.941573	1078.224382	14.181760
18.146366	1084.679166	14.186778
17.862998	1096.936383	14.191795
18.054739	1108.494728	14.196813
18.241307	1121.195278	14.201831
18.304329	1118.891036	14.206848
18.768190	1104.043735	14.211866
18.691646	1110.050520	14.216883
18.475966	1121.803348	14.221901
18.543582	1105.203331	14.226919
18.369858	1103.774687	14.231936
18.736910	1102.298401	14.236954
18.224171	1101.385743	14.241971
18.313174	1113.933148	14.246989
18.754913	1107.090114	14.252007
18.794360	1109.889099	14.257024
18.577757	1089.872090	14.262042
18.303578	1092.032862	14.267059
18.185176	1091.297713	14.272077
18.701607	1110.015736	14.277095
18.533880	1118.317718	14.282112
18.613519	1112.841385	14.287130
18.958692	1126.656285	14.292147
18.735436	1116.718367	14.297165
19.195803	1107.166216	14.302183
18.690988	1101.900233	14.307200
18.561931	1088.606391	14.312218
18.594139	1076.860443	14.317235
18.485133	1098.247117	14.322253
18.778427	1093.074796	14.327271
18.708347	1102.044373	14.332288
18.916111	1102.403945	14.337306
18.987970	1124.981622	14.342323
18.926762	1109.346825	14.347341
18.940092	1095.905058	14.352359
18.969209	1109.891050	14.357376
18.919678	1103.990670	14.362394
18.764815	1090.250381	14.367411
18.712780	1110.788037	14.372429
19.008934	1115.316151	14.377447
18.564453	1118.776705	14.382464
18.735791	1114.370074	14.387482
18.784006	1116.003046	14.392499
18.875260	1121.950615	14.397517
18.938418	1113.699917	14.402535
18.968272	1104.564524	14.407552
18.889724	1116.795585	14.412570
18.823768	1120.792303	14.417587
19.016967	1116.112616	14.422605
18.888524	1118.152868	14.427623
18.823594	1132.714367	14.432640
19.007025	1128.162844	14.437658
19.428909	1146.303723	14.442675
19.275707	1151.094461	14.447693
19.724397	1137.231164	14.452711
19.541799	1132.024895	14.457728
19.192577	1111.705025	14.462746
19.393002	1117.762482	14.467763
19.550685	1113.315989	14.472781
19.355071	1106.463734	14.477799
19.095818	1112.796333	14.482816
19.271534	1111.324309	14.487834
19.069825	1107.968334	14.492851
18.756894	1111.117629	14.497869
19.560242	1120.876183	14.502887
19.415813	1144.903960	14.507904
19.454759	1146.868727	14.512922
19.504034	1139.241858	14.517939
19.587153	1141.251481	14.522957
19.650979	1130.713645	14.527975
19.470163	1120.256790	14.532992
19.356419	1117.246845	14.538010
19.274045	1133.680990	14.543027
19.226223	1132.845213	14.548045
19.722879	1129.226211	14.553063
19.273785	1140.948347	14.558080
19.327150	1136.054991	14.563098
19.304634	1134.829271	14.568115
19.233392	1145.877063	14.573133
19.230989	1128.529074	14.578151
19.409982	1141.546194	14.583168
19.586766	1163.332308	14.588186
19.836223	1171.642331	14.593203
19.690631	1167.135330	14.598221
20.141237	1160.256560	14.603239
20.071793	1167.623188	14.608256
19.721199	1140.449725	14.613274
19.826463	1130.594100	14.618291
19.515200	1143.013614	14.623309
19.789666	1150.106113	14.628327
19.955750	1162.911248	14.633344
20.047801	1158.084315	14.638362
19.879792	1162.346686	14.643379
20.096188	1170.360451	14.648397
20.192681	1157.526831	14.653415
19.990759	1146.199576	14.658432
19.934856	1142.936604	14.663450
20.005561	1148.127471	14.668467
20.151502	1156.369961	14.673485
20.233381	1149.734974	14.678503
19.892341	1141.570936	14.683520
19.970677	1137.114718	14.688538
20.358040	1166.102027	14.693555
19.928293	1156.163371	14.698573
20.474002	1151.895222	14.703591
20.128328	1149.158402	14.708608
19.571859	1137.637031	14.713626
20.242049	1145.681875	14.718643
20.348984	1153.704667	14.723661
20.406725	1156.851957	14.728679
20.069976	1158.771349	14.733696
20.235810	1163.344238	14.738714
20.180495	1167.163058	14.743731
20.123407	1156.765836	14.748749
19.970034	1156.713318	14.753767
20.301121	1160.300986	14.758784
20.474107	1150.528825	14.763802
20.381026	1153.525085	14.768819
20.593442	1158.000919	14.773837
20.735713	1147.247583	14.778855
20.726226	1161.043184	14.783872
20.163779	1158.895243	14.788890
20.589158	1162.176432	14.793907
20.438733	1160.526056	14.798925
20.515200	1151.565381	14.803943
20.581883	1149.136928	14.808960
20.734128	1154.525310	14.813978
20.923478	1150.259369	14.818995
20.545420	1166.288749	14.824013
20.379379	1156.407874	14.829031
20.575761	1159.982966	14.834048
20.603309	1156.891603	14.839066
20.906256	1154.959448	14.844083
20.353149	1155.243810	14.849101
20.432992	1153.605766	14.854119
20.713357	1149.212992	14.859136
20.295376	1160.672171	14.864154
20.494093	1157.839283	14.869171
20.639654	1154.857727	14.874189
20.817895	1167.102681	14.879207
20.982088	1182.135727	14.884224
20.731123	1183.561891	14.889242
20.919007	1173.223961	14.894259
20.522574	1184.565245	14.899277
21.439022	1169.040628	14.904295
21.372627	1169.555136	14.909312
20.707446	1164.556144	14.914330
21.469161	1157.676741	14.919347
20.772035	1146.861959	14.924365
21.097000	1146.332034	14.929383
21.291644	1158.282390	14.934400
21.076865	1144.108327	14.939418
21.122822	1133.855482	14.944435
20.691385	1150.074738	14.949453
21.251971	1142.087235	14.954471
21.121017	1153.031337	14.959488
20.805661	1158.893582	14.964506
21.048269	1160.679836	14.969523
21.231367	1165.248691	14.974541
21.302907	1164.390235	14.979559
21.479616	1173.536751	14.984576
21.070358	1175.604916	14.989594
21.431490	1164.607954	14.994611
21.137673	1176.104686	14.999629
21.207582	1176.762389	15.004647
21.394576	1172.238607	15.009664
21.131257	1180.261980	15.014682
21.439989	1165.101532	15.019699
21.404834	1170.905471	15.024717
21.251935	1173.639617	15.029735
21.540063	1168.330155	15.034752
21.151843	1164.036057	15.039770
21.162065	1165.828239	15.044787
21.282043	1174.182493	15.049805
21.222222	1168.882902	15.054823
21.377572	1167.973003	15.059840
21.271907	1192.268812	15.064858
21.688683	1192.960715	15.069875
21.639563	1207.166974	15.074893
21.505465	1198.318419	15.079911
21.893233	1208.200226	15.084928
21.764510	1197.585521	15.089946
22.078692	1193.942534	15.094963
21.736079	1189.751306	15.099981
21.766827	1169.374471	15.104999
21.620485	1168.872047	15.110016
21.621006	1197.802104	15.115034
21.898403	1191.528622	15.120051
21.632381	1191.528179	15.125069
21.807702	1200.226588	15.130087
22.098659	1195.095361	15.135104
21.967428	1203.270904	15.140122
22.064088	1208.046546	15.145139
21.789194	1206.498413	15.150157
21.789766	1199.949467	15.155175
21.925718	1204.511954	15.160192
21.529743	1199.209253	15.165210
21.933637	1191.036041	15.170227
22.032151	1201.933989	15.175245
21.959794	1202.232590	15.180263
22.389719	1192.571460	15.185280
21.906094	1207.170731	15.190298
22.072796	1198.630676	15.195315
21.695701	1204.905831	15.200333
21.820072	1199.268754	15.205351
22.158701	1192.710788	15.210368
22.387151	1194.901682	15.215386
22.280438	1198.140517	15.220403
22.044558	1201.263714	15.225421
21.963629	1198.604768	15.230439
22.075027	1196.995357	15.235456
21.842281	1192.501373	15.240474
22.314808	1216.203326	15.245491
22.261423	1221.562928	15.250509
22.672308	1218.428279	15.255527
22.926094	1213.168564	15.260544
22.672529	1210.236816	15.265562
22.646891	1194.285082	15.270579
22.568102	1188.701855	15.275597
22.478966	1196.562418	15.280615
22.966517	1194.314563	15.285632
22.452963	1187.601610	15.290650
22.920698	1188.269149	15.295667
22.915137	1188.142606	15.300685
22.628624	1191.757749	15.305703
22.706004	1187.474678	15.310720
22.487894	1195.566756	15.315738
22.573569	1183.499934	15.320755
22.708732	1191.171681	15.325773
22.336482	1192.017987	15.330791
22.825639	1187.973706	15.335808
22.326254	1199.977971	15.340826
22.699009	1187.003806	15.345843
22.570233	1187.630772	15.350861
22.608205	1187.563362	15.355879
22.756584	1183.184911	15.360896
22.887265	1199.881704	15.365914
23.006953	1201.342467	15.370931
22.872767	1188.797688	15.375949
22.716381	1194.262280	15.380967
22.929016	1189.800582	15.385984
22.664546	1213.597361	15.391002
22.906944	1216.663369	15.396019
22.994648	1222.890062	15.401037
22.839249	1224.945607	15.406055
23.172408	1219.342906	15.411072
23.153825	1215.982821	15.416090
22.987652	1212.995693	15.421107
23.264198	1223.642815	15.426125
22.896224	1217.370873	15.431143
22.970084	1209.490932	15.436160
23.067721	1222.355648	15.441178
23.148566	1216.012095	15.446195
23.509429	1211.489681	15.451213
23.007819	1215.700521	15.456231
23.222757	1214.765224	15.461248
22.798607	1215.789569	15.466266
22.815564	1222.049800	15.471283
22.943107	1220.218463	15.476301
23.175688	1235.608310	15.481319
23.386303	1245.370425	15.486336
23.389047	1252.114435	15.491354
23.700952	1248.418671	15.496371
23.919931	1236.578360	15.501389
23.655085	1228.411131	15.506407
23.877845	1211.798941	15.511424
23.314718	1210.984745	15.516442
23.664380	1206.531102	15.521459
23.794853	1204.727427	15.526477
23.338119	1210.149942	15.531495
23.668190	1205.400176	15.536512
23.574604	1206.288803	15.541530
23.356932	1214.034222	15.546547
23.464333	1206.363271	15.551565
23.649872	1218.400796	15.556583
23.923260	1213.423229	15.561600
23.679300	1209.012772	15.566618
23.550216	1210.743547	15.571635
23.604462	1232.900543	15.576653
23.627260	1242.430548	15.581671
24.169781	1240.139552	15.586688
24.021266	1249.942321	15.591706
24.066994	1237.168197	15.596723
23.921588	1227.907978	15.601741
23.736002	1217.973807	15.606759
23.527438	1222.443455	15.611776
23.491184	1238.523690	15.616794
24.018263	1238.579946	15.621811
23.915922	1238.700265	15.626829
23.777929	1235.431354	15.631847
23.913154	1232.168859	15.636864
23.829258	1241.657647	15.641882
23.640819	1243.061477	15.646899
23.939040	1235.542216	15.651917
23.797520	1247.823151	15.656935
24.199933	1252.745097	15.661952
24.066134	1257.792266	15.666970
24.169688	1269.666242	15.671987
24.310864	1266.315762	15.677005
24.086657	1263.869428	15.682023
24.293157	1269.024314	15.687040
24.230201	1266.877658	15.692058
24.326153	1260.927393	15.697075
24.444219	1266.441325	15.702093
24.261125	1268.677212	15.707111
24.290792	1260.463067	15.712128
24.157752	1264.679537	15.717146
24.213963	1265.362536	15.722163
24.291407	1260.983976	15.727181
24.202237	1270.808836	15.732199
24.552834	1270.043409	15.737216
24.335532	1272.123361	15.742234
24.391955	1275.993220	15.747251
24.865648	1282.790104	15.752269
24.731984	1283.326164	15.757287
24.813952	1277.196539	15.762304
24.434331	1271.344740	15.767322
24.579998	1274.426942	15.772339
24.863061	1288.120579	15.777357
24.512802	1292.476480	15.782375
25.123305	1280.635794	15.787392
25.021321	1284.360993	15.792410
24.784548	1271.609710	15.797427
24.866966	1258.258533	15.802445
24.945902	1265.015544	15.807463
25.080499	1240.060372	15.812480
25.048326	1245.810902	15.817498
24.952604	1257.429067	15.822515
25.015740	1256.709768	15.827533
25.130562	1253.107192	15.832551
25.196248	1245.971967	15.837568
25.001162	1258.881940	15.842586
24.873133	1245.776737	15.847603
24.724203	1248.393921	15.852621
24.712295	1260.913642	15.857639
25.122955	1269.291159	15.862656
24.961285	1285.629336	15.867674
25.041130	1288.615348	15.872691
25.418240	1286.751224	15.877709
25.328059	1287.742230	15.882727
25.430712	1282.006169	15.887744
25.309258	1283.814418	15.892762
25.649034	1283.662297	15.897779
25.419054	1262.689747	15.902797
25.125826	1263.237413	15.907815
25.079266	1248.686297	15.912832
24.955266	1263.922143	15.917850
25.434477	1286.759263	15.922867
25.392999	1278.222863	15.927885
25.218908	1291.053814	15.932903
25.379119	1285.655626	15.937920
25.564093	1285.794595	15.942938
25.236564	1290.313248	15.947955
25.626146	1289.486663	15.952973
25.490369	1293.063536	15.957991
25.561324	1287.992647	15.963008
25.510055	1278.661731	15.968026
25.675966	1279.298654	15.973043
25.645714	1287.400083	15.978061
25.390343	1287.198305	15.983079
25.863592	1280.639311	15.988096
25.787064	1282.790474	15.993114
25.313683	1283.448215	15.998131
25.572617	1284.906444	16.003149
25.476208	1305.060810	16.008167
26.202991	1300.430663	16.013184
26.015187	1323.035403	16.018202
25.964179	1321.602007	16.023219
26.268197	1299.564148	16.028237
25.531553	1298.681196	16.033255
25.941289	1306.866593	16.038272
25.953154	1305.213196	16.043290
26.199663	1321.672510	16.048307
26.227273	1303.339595	16.053325
26.122019	1314.887933	16.058343
25.802105	1307.069867	16.063360
26.017263	1305.010295	16.068378
25.850087	1306.406877	16.073395
26.118426	1305.258845	16.078413
26.006372	1296.811252	16.083431
26.110986	1301.818445	16.088448
26.169785	1309.105295	16.093466
26.228626	1303.573090	16.098483
26.282028	1303.569261	16.103501
26.068498	1312.847268	16.108519
26.191028	1300.596733	16.113536
26.457626	1308.146046	16.118554
26.170044	1303.325317	16.123571
26.381722	1298.725776	16.128589
25.962555	1307.656327	16.133607
26.289084	1322.153511	16.138624
26.621456	1331.468462	16.143642
26.497463	1338.877055	16.148659
27.024258	1337.304872	16.153677
26.748574	1335.505517	16.158695
26.652745	1332.136128	16.163712
26.690098	1321.525384	16.168730
26.754182	1321.922483	16.173747
26.976956	1318.532134	16.178765
26.467816	1306.387555	16.183783
26.844715	1308.037873	16.188800
26.714340	1304.385465	16.193818
26.800214	1304.936221	16.198835
26.797313	1304.128243	16.203853
26.748852	1317.334455	16.208871
26.614832	1323.989108	16.213888
26.949875	1323.355559	16.218906
26.755106	1329.403224	16.223923
26.976232	1336.482188	16.228941
26.691009	1330.478567	16.233959
26.701354	1330.490710	16.238976
26.879692	1324.419342	16.243994
26.801042	1322.130215	16.249011
26.956725	1330.770143	16.254029
26.777495	1332.410612	16.259047
26.874528	1326.578234	16.264064
27.042823	1324.242590	16.269082
27.112286	1328.928093	16.274099
27.195299	1320.260288	16.279117
27.150212	1330.745710	16.284135
27.303585	1340.334303	16.289152
27.484201	1344.528090	16.294170
27.433935	1344.681136	16.299187
27.496375	1328.272846	16.304205
27.209008	1333.011414	16.309223
27.142086	1330.812262	16.314240
27.722058	1328.885283	16.319258
27.337976	1337.915155	16.324275
27.751582	1334.981183	16.329293
27.274251	1336.671111	16.334311
27.114513	1336.046505	16.339328
27.396867	1355.765961	16.344346
27.037528	1361.591463	16.349363
27.873512	1344.127907	16.354381
27.913984	1359.730110	16.359399
27.676720	1359.995148	16.364416
27.767113	1352.583786	16.369434
27.672732	1360.414202	16.374451
28.080325	1347.934855	16.379469
27.960020	1352.624762	16.384487
27.740956	1350.509993	16.389504
28.076587	1356.486156	16.394522
27.868705	1357.362975	16.399539
27.903963	1342.590998	16.404557
27.894720	1356.974438	16.409575
27.699563	1353.082369	16.414592
27.969080	1344.570905	16.419610
28.009422	1356.223934	16.424627
27.815863	1358.203532	16.429645
27.839255	1347.696635	16.434663
27.904655	1358.061471	16.439680
27.969427	1351.994688	16.444698
27.835523	1354.007334	16.449715
28.141992	1353.934524	16.454733
27.954279	1355.029630	16.459751
27.946890	1344.436695	16.464768
28.451776	1356.451864	16.469786
28.084064	1358.695639	16.474803
28.353935	1348.373762	16.479821
28.338850	1340.351194	16.484839
28.211415	1357.439184	16.489856
28.179825	1351.939029	16.494874
27.790131	1362.293851	16.499891
28.260970	1375.343047	16.504909
28.076796	1381.122682	16.509927
28.152201	1388.766024	16.514944
28.202175	1376.894094	16.519962
28.127373	1385.517623	16.524979
28.122488	1387.716401	16.529997
28.675642	1387.994891	16.535015
28.453498	1401.868757	16.540032
28.534590	1407.275088	16.545050
28.784580	1411.607800	16.550067
28.842419	1403.607198	16.555085
29.151898	1397.701502	16.560103
28.953752	1379.677810	16.565120
28.934394	1365.212035	16.570138
28.875014	1376.462726	16.575155
28.996571	1372.226428	16.580173
28.956944	1369.973359	16.585191
28.832856	1369.869944	16.590208
28.991027	1365.972624	16.595226
29.016319	1370.607377	16.600243
29.355073	1371.217315	16.605261
29.336075	1372.152672	16.610279
29.309781	1366.601643	16.615296
29.472233	1372.007113	16.620314
28.937550	1368.254207	16.625331
29.066960	1370.299707	16.630349
29.405398	1369.313288	16.635367
29.160677	1373.858432	16.640384
29.642657	1366.524455	16.645402
29.263614	1361.853053	16.650419
28.886164	1348.071375	16.655437
29.208961	1364.564775	16.660455
29.153392	1370.039733	16.665472
29.328905	1367.614911	16.670490
29.009123	1370.592386	16.675507
29.003372	1368.361076	16.680525
29.137718	1373.292524	16.685543
29.055282	1370.519051	16.690560
29.419278	1369.082610	16.695578
29.245638	1369.104886	16.700595
29.339585	1376.882341	16.705613
29.418892	1380.209747	16.710631
29.649453	1402.818684	16.715648
29.489898	1389.953376	16.720666
29.712618	1396.535920	16.725683
29.283794	1410.677378	16.730701
29.701483	1408.262719	16.735719
29.332377	1405.597430	16.740736
29.624238	1392.737430	16.745754
29.426748	1400.192839	16.750771
29.468095	1415.265506	16.755789
29.507076	1392.303741	16.760807
29.622075	1412.675833	16.765824
29.938627	1424.918212	16.770842
30.485851	1434.351438	16.775859
30.398613	1411.741555	16.780877
30.182793	1410.288741	16.785895
29.926793	1403.695113	16.790912
30.092291	1401.773834	16.795930
29.785290	1390.167548	16.800947
29.728091	1388.863102	16.805965
30.122460	1410.301060	16.810983
30.018658	1409.917956	16.816000
30.363282	1421.091287	16.821018
30.120372	1428.153291	16.826035
30.477770	1419.813062	16.831053
30.590142	1418.970675	16.836071
30.311119	1434.819621	16.841088
30.450110	1426.176753	16.846106
30.309559	1420.716032	16.851123
30.775758	1419.117641	16.856141
30.300844	1395.126593	16.861159
30.004811	1405.651961	16.866176
30.190425	1418.701879	16.871194
30.443307	1429.341837	16.876211
30.192121	1419.120389	16.881229
30.403288	1419.129854	16.886247
30.472726	1424.173998	16.891264
30.603378	1413.016946	16.896282
30.166023	1427.482419	16.901299
30.525996	1430.072415	16.906317
30.575396	1426.565243	16.911335
30.581082	1431.404996	16.916352
30.873254	1444.070846	16.921370
30.881403	1430.029535	16.926387
30.927508	1442.359726	16.931405
31.445054	1428.190344	16.936423
30.800489	1435.272278	16.941440
31.122954	1421.335505	16.946458
30.650561	1427.172235	16.951475
30.564070	1423.683977	16.956493
31.067369	1441.624970	16.961511
31.044919	1436.467514	16.966528
30.885579	1442.889036	16.971546
31.169343	1459.045928	16.976563
31.247473	1456.502953	16.981581
31.347316	1452.636703	16.986599
31.196002	1451.681221	16.991616
31.599354	1456.802655	16.996634
31.579599	1430.340231	17.001651
31.132623	1430.992826	17.006669
31.196706	1415.606066	17.011687
30.791182	1431.596566	17.016704
31.013865	1442.225187	17.021722
31.327118	1435.708708	17.026739
31.167989	1449.943211	17.031757
31.491790	1455.353538	17.036775
31.297495	1449.033510	17.041792
31.469477	1443.988585	17.046810
31.469427	1450.821714	17.051827
31.271730	1451.410677	17.056845
31.419863	1449.329294	17.061863
31.282372	1461.716411	17.066880
31.530215	1468.511141	17.071898
31.644085	1475.766335	17.076915
31.764351	1478.112923	17.081933
31.791435	1470.943429	17.086951
31.888223	1473.940259	17.091968
32.148094	1475.748497	17.096986
31.729113	1474.169430	17.102003
31.868582	1483.302997	17.107021
32.023443	1471.507939	17.112039
31.779613	1478.045982	17.117056
31.968931	1468.741915	17.122074
32.149693	1477.504928	17.127091
31.586798	1480.285232	17.132109
31.779629	1473.631377	17.137127
32.066638	1478.654543	17.142144
32.412697	1476.179476	17.147162
32.140830	1463.321054	17.152179
31.871815	1476.919507	17.157197
32.329131	1472.042152	17.162215
32.120836	1473.856114	17.167232
32.234914	1473.461015	17.172250
32.366238	1474.842334	17.177267
32.209048	1492.835457	17.182285
32.604812	1500.686309	17.187303
32.649263	1497.503711	17.192320
32.699745	1484.384747	17.197338
32.620428	1474.331485	17.202355
32.341106	1459.371653	17.207373
32.682901	1463.675825	17.212391
32.427565	1475.206572	17.217408
32.563176	1468.497420	17.222426
32.895452	1478.933572	17.227443
32.791426	1481.916745	17.232461
32.816110	1464.032286	17.237479
32.377759	1467.240759	17.242496
32.787227	1465.969210	17.247514
32.855021	1482.437762	17.252531
32.781131	1475.961821	17.257549
32.965131	1478.862755	17.262567
33.179498	1486.786090	17.267584
32.866531	1466.349735	17.272602
32.767299	1465.100647	17.277619
32.614972	1473.172748	17.282637
33.242705	1475.934221	17.287655
33.130070	1478.087441	17.292672
33.261670	1481.444018	17.297690
33.243853	1474.849181	17.302707
33.181514	1478.779656	17.307725
33.154801	1481.357787	17.312743
33.084320	1479.764233	17.317760
33.085875	1484.961720	17.322778
33.320517	1481.621533	17.327795
33.119387	1472.577628	17.332813
33.530818	1475.831471	17.337831
33.352237	1486.683104	17.342848
33.225937	1480.675795	17.347866
33.506798	1485.290394	17.352883
33.333231	1489.343765	17.357901
33.654585	1484.273944	17.362919
33.558857	1476.758260	17.367936
33.254597	1481.401057	17.372954
33.561569	1489.511423	17.377971
33.731723	1488.356182	17.382989
33.704413	1483.545919	17.388007
33.145778	1487.995947	17.393024
33.657547	1482.271719	17.398042
34.004945	1488.775440	17.403059
33.811526	1492.286109	17.408077
34.107151	1473.894725	17.413095
33.471957	1491.639919	17.418112
33.720263	1507.465173	17.423130
34.165110	1503.945972	17.428147
33.870028	1517.008295	17.433165
34.168401	1500.513398	17.438183
34.254142	1501.590093	17.443200
34.080932	1504.144412	17.448218
34.434754	1501.554296	17.453235
33.747398	1490.206431	17.458253
34.204572	1508.995554	17.463271
34.314118	1511.321088	17.468288
34.296956	1499.109224	17.473306
34.502295	1503.490281	17.478323
34.165279	1510.556262	17.483341
34.343750	1514.502455	17.488359
34.437838	1500.380548	17.493376
33.958505	1507.628881	17.498394
34.368178	1500.950005	17.503411
34.145863	1503.429184	17.508429
34.556905	1500.099206	17.513447
34.657912	1493.037940	17.518464
34.419282	1488.979816	17.523482
34.482689	1496.785998	17.528499
34.234736	1496.806973	17.533517
34.702952	1489.937745	17.538535
35.001561	1496.849080	17.543552
34.594187	1494.577839	17.548570
34.622417	1499.865791	17.553587
34.406692	1504.001713	17.558605
34.813732	1507.693234	17.563623
34.917995	1521.851802	17.568640
34.900125	1523.789791	17.573658
35.258080	1513.822683	17.578675
35.009925	1511.277525	17.583693
35.198935	1516.320244	17.588711
35.230502	1502.519844	17.593728
35.001834	1492.138152	17.598746
35.015600	1499.405767	17.603763
35.285870	1503.486175	17.608781
34.862051	1497.425284	17.613799
34.967872	1500.293086	17.618816
35.073144	1511.807372	17.623834
35.103675	1507.867929	17.628851
35.065853	1520.739338	17.633869
35.021679	1510.063797	17.638887
35.169524	1512.570967	17.643904
34.819228	1524.924808	17.648922
35.171863	1513.450528	17.653939
35.096118	1535.617830	17.658957
35.086222	1542.697081	17.663975
35.555095	1542.170524	17.668992
35.113020	1542.400129	17.674010
35.471188	1543.753021	17.679027
35.354681	1549.060382	17.684045
35.493529	1553.238691	17.689063
35.941904	1547.570382	17.694080
35.997613	1555.558746	17.699098
35.647559	1538.040218	17.704115
35.766709	1541.126266	17.709133
35.824126	1552.108212	17.714151
35.901889	1566.072213	17.719168
36.083710	1568.931404	17.724186
36.326488	1560.128809	17.729203
36.039964	1553.838544	17.734221
36.026891	1539.735885	17.739239
36.147931	1547.932512	17.744256
36.127233	1549.529877	17.749274
36.131026	1557.716558	17.754291
36.309480	1570.622141	17.759309
36.379561	1558.428486	17.764327
36.314765	1550.929501	17.769344
36.543442	1543.398358	17.774362
36.367544	1538.219382	17.779379
36.300611	1535.394308	17.784397
36.024236	1542.432174	17.789415
36.480584	1555.944878	17.794432
36.639494	1581.877068	17.799450
36.441724	1564.226076	17.804467
36.581136	1567.552054	17.809485
36.339728	1572.802121	17.814503
36.584658	1558.664682	17.819520
36.620161	1568.562619	17.824538
36.781032	1568.400894	17.829555
36.846733	1566.512619	17.834573
36.693042	1564.207515	17.839591
37.096090	1562.951191	17.844608
36.732329	1566.357368	17.849626
36.853636	1555.491677	17.854643
37.041046	1559.930626	17.859661
36.686146	1552.144392	17.864679
36.828035	1556.819374	17.869696
36.850341	1556.572491	17.874714
36.971724	1554.999774	17.879731
36.733737	1557.617949	17.884749
36.826494	1548.704345	17.889767
37.342405	1563.035048	17.894784
36.894031	1563.231250	17.899802
37.391764	1570.177223	17.904819
37.530554	1578.753556	17.909837
37.265070	1568.330856	17.914855
37.261376	1570.318469	17.919872
37.309699	1589.976326	17.924890
37.475037	1582.568017	17.929907
37.517676	1587.873104	17.934925
37.248108	1598.310777	17.939943
37.450166	1585.183016	17.944960
37.564980	1594.522073	17.949978
37.376322	1592.887021	17.954995
37.429403	1590.345211	17.960013
37.493850	1591.314816	17.965031
37.489060	1584.437307	17.970048
37.506289	1588.852230	17.975066
37.698994	1581.282925	17.980083
37.591347	1585.283307	17.985101
37.756080	1584.215360	17.990119
38.021397	1588.151747	17.995136
37.526432	1590.202834	18.000154
37.643398	1579.853913	18.005171
37.944532	1600.650549	18.010189
38.135548	1605.209568	18.015207
38.106551	1605.665752	18.020224
37.969863	1620.336408	18.025242
38.282927	1611.893772	18.030259
38.176610	1607.659639	18.035277
38.343115	1608.370877	18.040295
38.326946	1598.321860	18.045312
38.112096	1604.315478	18.050330
38.337367	1599.236305	18.055347
38.396691	1611.635106	18.060365
38.304624	1599.525884	18.065383
38.457387	1593.469659	18.070400
38.216504	1602.066824	18.075418
38.353013	1600.702204	18.080435
38.294625	1603.587123	18.085453
38.234294	1604.153195	18.090471
38.547540	1598.625489	18.095488
38.470794	1624.860044	18.100506
38.863263	1621.937385	18.105523
38.957738	1623.499586	18.110541
38.859605	1623.291894	18.115559
38.566543	1600.587418	18.120576
38.758261	1632.631540	18.125594
38.753160	1629.892674	18.130611
38.953372	1635.192995	18.135629
39.005218	1629.579752	18.140647
39.349176	1630.148887	18.145664
39.079312	1630.664361	18.150682
39.173561	1630.496718	18.155699
39.334294	1628.632096	18.160717
39.158981	1620.011338	18.165735
39.239570	1631.131816	18.170752
39.040503	1631.708809	18.175770
39.320795	1624.920963	18.180787
38.989945	1630.124816	18.185805
39.205069	1640.261977	18.190823
39.544798	1627.623565	18.195840
39.160307	1639.145860	18.200858
39.093172	1645.396344	18.205875
39.317793	1628.227174	18.210893
39.217955	1630.759548	18.215911
39.533808	1629.417840	18.220928
39.662501	1643.088099	18.225946
39.555216	1660.732470	18.230963
39.536729	1660.732058	18.235981
39.530073	1650.463550	18.240999
39.934078	1652.552478	18.246016
39.624079	1660.609401	18.251034
39.710260	1648.585826	18.256051
39.958477	1650.367865	18.261069
39.989758	1650.555266	18.266087
40.311552	1645.636875	18.271104
40.066043	1652.946228	18.276122
40.174665	1647.108862	18.281139
40.326727	1654.078340	18.286157
39.978573	1651.369983	18.291175
39.971175	1641.266936	18.296192
39.882455	1651.036853	18.301210
40.078896	1645.146792	18.306227
40.169166	1644.311195	18.311245
40.187499	1653.592817	18.316263
40.331810	1641.046718	18.321280
40.476826	1645.614335	18.326298
40.469977	1647.599134	18.331315
40.518705	1641.446515	18.336333
40.443101	1633.257243	18.341351
40.202319	1638.507426	18.346368
40.397062	1641.889425	18.351386
40.591164	1665.380640	18.356403
41.031704	1668.574802	18.361421
40.600884	1680.275824	18.366439
41.074721	1668.743412	18.371456
40.895594	1656.488907	18.376474
41.058857	1644.254198	18.381491
41.102262	1630.698740	18.386509
40.850801	1640.167242	18.391527
41.233561	1629.316356	18.396544
40.979887	1634.482657	18.401562
41.212140	1631.429801	18.406579
41.161281	1635.504265	18.411597
40.796746	1637.678075	18.416615
40.882584	1623.781994	18.421632
41.031691	1651.177337	18.426650
41.070996	1666.000818	18.431667
41.416677	1663.167762	18.436685
41.226792	1667.691727	18.441703
41.317917	1669.387933	18.446720
41.262481	1666.842393	18.451738
41.237073	1673.182437	18.456755
41.541950	1670.295501	18.461773
41.407311	1663.836212	18.466791
41.219819	1668.562904	18.471808
41.277905	1678.214496	18.476826
40.667776	1671.657229	18.481843
41.326235	1681.975256	18.486861
41.694559	1697.305345	18.491879
41.980498	1695.681802	18.496896
41.893114	1694.176243	18.501914
41.326893	1701.307742	18.506931
41.882585	1697.168883	18.511949
41.664918	1688.763522	18.516967
41.623245	1691.839174	18.521984
41.985575	1706.364267	18.527002
41.764511	1712.196179	18.532019
42.225660	1721.009835	18.537037
42.440834	1723.422657	18.542055
42.697149	1719.956805	18.547072
42.537220	1704.926812	18.552090
42.427229	1694.772582	18.557107
42.245356	1687.314529	18.562125
42.128181	1686.768492	18.567143
42.122874	1695.028000	18.572160
42.026457	1708.643011	18.577178
42.301571	1714.331323	18.582195
42.957116	1702.918052	18.587213
42.611080	1718.681526	18.592231
42.850056	1718.843068	18.597248
42.944842	1708.933693	18.602266
42.525831	1722.670127	18.607283
42.693991	1713.704602	18.612301
42.806996	1716.698997	18.617319
42.627531	1712.927651	18.622336
42.676728	1705.109398	18.627354
42.980568	1716.875042	18.632371
42.673752	1696.498772	18.637389
42.820022	1705.230022	18.642407
42.751984	1708.062626	18.647424
43.237256	1711.588139	18.652442
43.080672	1710.626032	18.657459
43.070971	1705.447680	18.662477
42.739761	1715.492522	18.667495
42.878966	1709.571939	18.672512
42.959589	1714.263983	18.677530
42.907227	1728.748782	18.682547
43.209475	1732.241365	18.687565
43.217747	1745.763134	18.692583
43.412325	1726.115478	18.697600
43.407595	1734.616810	18.702618
43.353574	1739.495066	18.707635
43.464424	1736.186894	18.712653
43.629670	1738.017691	18.717671
43.321078	1732.451378	18.722688
43.195463	1734.803800	18.727706
43.346619	1750.007253	18.732723
43.697295	1753.010403	18.737741
43.511910	1751.987903	18.742759
43.629048	1756.854808	18.747776
44.182636	1756.075301	18.752794
44.092061	1763.707286	18.757811
44.237444	1753.529909	18.762829
44.257549	1748.485182	18.767847
44.117673	1759.844915	18.772864
44.545798	1746.457246	18.777882
44.667428	1751.855622	18.782899
44.575516	1742.536061	18.787917
44.323507	1733.050664	18.792935
44.304154	1718.892981	18.797952
44.486227	1712.612209	18.802970
44.220072	1722.965751	18.807987
44.493383	1717.675872	18.813005
44.492491	1742.211107	18.818023
44.456297	1752.454236	18.823040
44.917197	1747.141614	18.828058
44.650856	1738.637984	18.833075
44.572450	1729.745868	18.838093
44.678377	1726.401902	18.843111
44.590401	1741.260267	18.848128
44.475727	1747.130116	18.853146
44.806068	1751.124099	18.858163
45.065538	1751.974293	18.863181
44.658933	1749.299000	18.868199
45.116155	1751.633446	18.873216
44.876515	1748.764834	18.878234
44.660634	1750.725929	18.883251
44.640019	1744.220995	18.888269
44.796998	1743.746959	18.893287
44.746271	1751.767185	18.898304
45.350720	1762.125881	18.903322
45.225246	1775.745162	18.908339
45.331536	1773.925736	18.913357
45.323222	1776.055263	18.918375
45.344857	1776.984913	18.923392
45.490947	1783.599773	18.928410
45.199173	1781.414489	18.933427
45.357893	1773.358839	18.938445
45.327651	1780.801752	18.943463
45.306756	1776.636320	18.948480
45.565850	1779.015321	18.953498
45.088262	1785.803513	18.958515
45.877630	1782.964036	18.963533
45.424826	1793.984217	18.968551
45.682627	1801.672614	18.973568
46.003374	1807.605356	18.978586
45.807480	1812.454332	18.983603
45.982017	1815.201992	18.988621
45.773360	1810.363139	18.993639
45.588711	1815.079170	18.998656
46.007825	1811.362801	19.003674
46.031227	1802.597502	19.008691
46.086251	1803.176207	19.013709
45.936440	1806.781499	19.018727
46.026223	1805.093128	19.023744
46.455534	1808.415538	19.028762
46.175653	1827.122153	19.033779
46.814908	1833.396121	19.038797
46.571222	1814.643903	19.043815
46.488165	1813.913899	19.048832
46.415032	1800.061448	19.053850
46.431653	1818.158102	19.058867
46.878192	1837.803021	19.063885
46.890208	1828.267440	19.068903
46.761731	1832.081784	19.073920
47.035237	1825.227855	19.078938
46.863140	1830.380936	19.083955
46.879646	1829.353804	19.088973
46.992474	1835.173297	19.093991
46.865930	1823.460296	19.099008
47.254379	1817.885837	19.104026
47.149340	1834.672268	19.109043
46.752913	1818.001924	19.114061
46.940006	1822.143008	19.119079
46.854474	1821.654131	19.124096
47.197159	1814.924584	19.129114
47.034974	1819.574314	19.134131
47.286004	1810.730061	19.139149
47.050774	1805.480888	19.144167
47.579073	1825.331151	19.149184
47.436624	1825.275249	19.154202
46.850556	1830.711477	19.159219
47.265267	1844.517503	19.164237
47.840323	1849.025728	19.169255
47.641918	1842.046061	19.174272
48.035466	1841.827381	19.179290
47.939005	1844.020297	19.184307
48.106751	1845.258836	19.189325
48.184006	1836.238389	19.194343
48.221858	1841.784089	19.199360
48.227917	1831.386997	19.204378
48.116877	1841.635665	19.209395
48.522699	1827.763875	19.214413
48.158828	1804.824765	19.219431
48.067252	1806.794652	19.224448
48.126933	1802.391712	19.229466
48.012697	1816.046963	19.234483
47.982334	1822.078673	19.239501
48.056706	1834.490914	19.244519
48.069167	1839.433010	19.249536
48.338023	1833.566733	19.254554
48.069829	1847.000436	19.259571
48.089596	1835.610251	19.264589
48.454116	1834.079010	19.269607
48.521255	1852.825150	19.274624
48.777192	1846.279195	19.279642
48.581973	1868.760189	19.284659
48.634774	1871.592142	19.289677
48.913395	1853.643812	19.294695
48.615896	1859.324454	19.299712
48.732883	1860.278505	19.304730
49.227250	1857.545829	19.309747
48.774909	1863.227654	19.314765
49.203150	1868.500805	19.319783
49.151481	1867.260751	19.324800
49.052729	1867.981589	19.329818
48.871417	1869.071342	19.334835
48.928335	1858.489274	19.339853
49.182501	1851.596014	19.344871
49.078917	1864.581322	19.349888
49.243149	1861.735897	19.354906
49.124522	1868.965337	19.359923
49.043153	1872.375104	19.364941
49.327162	1876.724963	19.369959
49.334352	1899.861250	19.374976
49.409566	1892.179335	19.379994
49.541367	1880.736749	19.385011
49.617298	1882.654558	19.390029
49.658110	1879.251446	19.395047
49.742942	1890.647952	19.400064
49.651222	1893.313263	19.405082
49.711142	1899.873327	19.410099
49.809331	1897.891071	19.415117
50.063969	1908.786751	19.420135
49.994110	1923.145309	19.425152
50.331432	1904.934295	19.430170
50.381192	1912.852773	19.435187
50.388488	1916.371506	19.440205
50.429913	1892.898807	19.445223
50.228854	1903.492471	19.450240
50.683112	1900.452870	19.455258
50.448305	1900.775179	19.460275
50.692402	1893.991033	19.465293
50.757787	1892.588540	19.470311
50.558927	1883.741434	19.475328
50.515842	1871.727236	19.480346
50.725823	1887.926102	19.485363
50.505802	1897.424404	19.490381
50.954016	1908.805750	19.495399
50.694753	1894.985349	19.500416
50.927144	1897.325677	19.505434
50.729104	1904.460198	19.510451
50.705891	1899.019478	19.515469
50.722601	1888.115333	19.520487
51.105985	1902.029724	19.525504
50.953637	1898.786072	19.530522
50.701761	1904.236974	19.535539
50.604084	1909.865127	19.540557
51.073104	1909.978422	19.545575
50.608721	1933.100376	19.550592
51.162819	1928.711355	19.555610
51.293480	1943.401123	19.560627
51.111756	1933.309175	19.565645
51.453311	1929.741799	19.570663
51.503585	1960.167847	19.575680
51.547999	1953.380259	19.580698
51.907754	1951.584077	19.585715
51.631048	1958.130313	19.590733
51.738908	1953.617412	19.595751
51.888844	1954.892955	19.600768
51.920075	1960.742710	19.605786
51.889549	1956.016484	19.610803
51.853079	1946.099713	19.615821
52.187869	1951.827853	19.620839
51.951082	1951.638148	19.625856
52.133237	1946.840561	19.630874
52.282108	1941.117088	19.635891
51.989790	1947.871192	19.640909
52.315434	1943.213852	19.645927
52.155430	1944.550454	19.650944
52.302718	1942.661839	19.655962
52.338541	1942.988240	19.660979
52.315264	1956.944099	19.665997
52.579661	1938.863586	19.671015
52.154899	1950.114847	19.676032
52.430527	1952.018757	19.681050
52.361549	1958.024425	19.686067
52.382102	1972.874723	19.691085
52.942926	1970.265282	19.696103
52.876681	1979.944105	19.701120
52.911096	1975.866121	19.706138
52.799158	1967.375033	19.711155
52.760672	1982.364020	19.716173
53.270083	1969.614817	19.721191
53.202971	1974.704539	19.726208
53.429007	1971.526871	19.731226
53.298132	1966.207845	19.736243
53.219133	1971.605795	19.741261
53.267226	1969.611732	19.746279
53.064983	1961.258785	19.751296
53.132846	1968.386792	19.756314
53.201467	1973.886515	19.761331
53.153835	1969.716591	19.766349
53.215518	1978.710569	19.771367
53.354540	2003.543142	19.776384
53.508118	1988.456734	19.781402
53.347141	1998.124257	19.786419
53.386377	2008.114173	19.791437
53.690743	2002.843669	19.796455
53.448743	2009.114734	19.801472
54.249549	2021.858999	19.806490
54.567161	2012.789872	19.811507
54.159937	2010.219740	19.816525
54.722162	1990.982593	19.821543
54.424540	1986.786661	19.826560
54.174341	1997.024770	19.831578
54.131512	1992.276749	19.836595
54.188620	1990.818338	19.841613
54.301346	1984.199940	19.846631
54.286308	1983.438611	19.851648
54.359469	2002.474456	19.856666
54.654472	2015.381032	19.861683
54.555649	2023.541026	19.866701
55.138668	2022.243709	19.871719
54.853425	2023.054223	19.876736
54.879429	2007.637145	19.881754
55.001922	2009.348479	19.886771
54.716106	2000.181657	19.891789
55.143452	1992.160824	19.896807
54.899551	2004.818296	19.901824
54.887981	2018.419953	19.906842
54.944175	2012.125416	19.911859
54.480824	2025.693285	19.916877
54.846458	2027.120767	19.921895
55.115506	2014.441363	19.926912
54.901468	2018.055940	19.931930
54.811386	2026.527841	19.936947
55.222770	2039.182948	19.941965
55.185552	2045.391253	19.946983
54.960349	2052.206743	19.952000
55.038782	2050.177345	19.957018
55.406290	2050.841414	19.962035
55.377934	2065.154471	19.967053
55.521528	2057.382638	19.972071
55.532913	2070.654205	19.977088
55.743830	2076.991382	19.982106
56.169522	2069.885645	19.987123
55.993139	2066.208378	19.992141
56.342833	2067.388525	19.997159
56.101381	2068.995065	20.002176
56.187520	2074.270497	20.007194
56.404432	2065.624038	20.012211
56.227268	2074.772490	20.017229
56.318370	2076.995461	20.022247
56.232597	2058.840405	20.027264
56.157086	2078.091836	20.032282
56.604525	2077.751072	20.037299
56.526889	2070.396263	20.042317
56.679888	2066.238429	20.047335
56.077931	2074.489466	20.052352
56.493234	2067.813354	20.057370
56.305768	2055.089683	20.062387
56.593015	2071.139768	20.067405
56.694613	2066.390886	20.072423
56.759546	2067.592897	20.077440
56.537694	2088.465990	20.082458
57.076552	2089.811906	20.087475
57.180563	2100.547397	20.092493
57.017836	2092.606111	20.097511
57.059265	2096.721542	20.102528
57.408871	2097.242328	20.107546
57.498503	2102.171165	20.112563
57.305166	2102.169729	20.117581
57.194601	2091.592345	20.122599
57.497699	2102.290411	20.127616
57.299137	2092.180277	20.132634
57.786213	2078.043485	20.137651
57.591444	2088.345518	20.142669
57.406072	2078.346981	20.147687
57.538508	2078.233843	20.152704
57.255393	2095.911113	20.157722
57.893649	2097.222496	20.162739
57.778022	2102.449398	20.167757
58.060926	2111.527553	20.172775
58.309953	2113.239837	20.177792
58.080246	2111.400313	20.182810
58.654394	2108.090296	20.187827
58.522861	2107.908783	20.192845
58.784231	2095.545705	20.197863
58.731933	2089.033658	20.202880
58.309090	2067.049076	20.207898
58.414297	2063.373893	20.212915
58.274303	2067.558859	20.217933
58.309802	2065.828058	20.222951
58.659932	2081.666997	20.227968
58.301336	2095.360710	20.232986
58.579986	2107.215453	20.238003
58.595859	2103.161757	20.243021
58.916893	2095.779240	20.248039
58.945419	2102.220969	20.253056
58.767293	2103.890269	20.258074
58.983695	2103.199141	20.263091
58.631254	2102.620911	20.268109
58.721512	2088.260345	20.273127
59.063887	2101.176880	20.278144
58.810017	2126.695773	20.283162
59.104696	2127.664961	20.288179
59.035732	2124.393703	20.293197
59.120028	2131.986147	20.298215
59.315454	2127.349484	20.303232
58.986611	2120.043249	20.308250
59.027449	2125.853492	20.313267
59.335605	2156.486696	20.318285
59.274880	2154.289158	20.323303
59.720057	2151.008711	20.328320
59.333863	2159.142847	20.333338
59.955623	2142.872734	20.338355
59.958110	2149.372323	20.343373
59.825010	2158.421426	20.348391
60.150295	2156.563995	20.353408
60.214402	2155.350844	20.358426
60.248643	2150.421748	20.363443
60.328416	2154.660570	20.368461
60.539051	2150.745919	20.373479
60.206662	2151.681542	20.378496
60.209154	2150.675797	20.383514
60.282455	2164.241512	20.388531
60.385091	2168.769444	20.393549
60.331982	2166.675753	20.398567
60.474211	2176.608802	20.403584
60.635447	2184.539900	20.408602
60.869793	2172.136350	20.413619
60.795652	2180.853512	20.418637
60.667305	2179.511351	20.423655
60.930658	2171.166380	20.428672
60.857121	2178.969163	20.433690
61.008848	2175.789562	20.438707
60.909524	2179.120286	20.443725
60.912002	2187.546668	20.448743
61.141442	2187.839308	20.453760
61.352888	2203.752663	20.458778
61.660722	2203.457011	20.463795
61.518760	2195.947040	20.468813
61.890463	2204.470866	20.473831
61.877618	2199.428878	20.478848
61.602828	2201.132270	20.483866
61.633119	2196.925591	20.488883
61.755012	2199.712136	20.493901
61.593449	2195.262780	20.498919
62.018329	2192.120902	20.503936
62.252203	2197.022391	20.508954
62.041083	2197.796651	20.513971
61.777732	2197.161770	20.518989
61.884105	2192.838987	20.524007
62.150310	2199.157630	20.529024
61.775217	2194.130825	20.534042
62.435332	2188.348169	20.539059
62.340509	2193.310272	20.544077
61.901606	2194.209960	20.549095
62.018763	2191.411818	20.554112
62.357944	2214.282714	20.559130
62.077733	2208.408023	20.564147
62.510832	2211.476771	20.569165
62.620422	2223.654592	20.574183
62.797432	2214.228894	20.579200
62.421696	2214.002113	20.584218
62.825212	2220.584463	20.589235
62.820602	2237.197468	20.594253
62.870573	2244.802726	20.599271
63.357579	2243.874374	20.604288
63.420343	2254.268200	20.609306
63.279255	2231.075517	20.614323
63.634614	2239.008026	20.619341
63.509246	2235.861015	20.624359
63.705038	2218.553644	20.629376
63.418285	2219.238838	20.634394
63.464078	2204.464687	20.639411
63.216184	2206.245713	20.644429
63.483977	2221.803353	20.649447
63.589252	2228.556830	20.654464
63.721131	2227.061241	20.659482
63.888147	2227.355733	20.664499
63.515124	2223.495392	20.669517
63.735384	2227.174653	20.674535
63.897889	2236.219044	20.679552
63.810110	2228.274357	20.684570
63.976816	2217.077894	20.689587
64.082322	2220.290535	20.694605
64.044079	2240.490641	20.699623
64.198727	2246.606697	20.704640
64.155100	2259.651714	20.709658
64.144070	2251.858686	20.714675
64.270833	2253.010341	20.719693
64.229429	2263.326120	20.724711
64.592125	2246.109039	20.729728
64.226134	2259.024666	20.734746
64.673268	2273.694733	20.739763
64.818698	2275.434784	20.744781
64.878040	2295.798544	20.749799
65.232716	2287.226235	20.754816
65.213839	2283.985049	20.759834
65.016165	2274.112027	20.764851
65.520140	2277.628482	20.769869
65.070166	2271.364143	20.774887
65.221579	2278.713307	20.779904
65.127466	2281.800695	20.784922
65.216168	2263.423277	20.789939
65.317946	2275.794340	20.794957
65.232241	2273.321412	20.799975
65.701483	2280.337373	20.804992
65.604919	2298.462546	20.810010
65.698770	2301.632842	20.815027
65.818967	2301.569753	20.820045
65.769973	2306.954595	20.825063
65.861643	2296.680233	20.830080
65.894522	2301.632685	20.835098
65.948848	2297.058064	20.840115
66.220211	2293.496695	20.845133
65.939090	2299.519444	20.850151
66.270877	2295.803614	20.855168
65.741165	2297.420610	20.860186
66.205722	2305.955721	20.865203
66.440507	2326.393080	20.870221
66.493835	2323.650340	20.875239
66.828594	2329.628408	20.880256
66.662000	2324.978485	20.885274
66.650758	2325.161898	20.890291
66.729550	2323.554611	20.895309
67.025253	2328.575047	20.900327
67.010737	2316.015673	20.905344
67.098309	2324.712098	20.910362
67.029494	2319.933627	20.915379
67.309737	2307.705438	20.920397
66.867462	2319.755062	20.925415
67.475429	2306.720817	20.930432
67.138118	2316.846576	20.935450
67.202463	2312.883034	20.940467
67.313030	2314.173971	20.945485
67.170950	2334.269914	20.950503
67.433180	2331.948713	20.955520
67.626009	2334.131684	20.960538
67.757059	2340.117044	20.965555
67.899003	2344.591095	20.970573
67.778492	2337.429250	20.975591
68.028415	2330.307563	20.980608
67.876056	2340.614566	20.985626
67.703394	2333.354855	20.990643
68.055984	2326.674627	20.995661
67.955107	2340.328724	21.000679
67.917499	2340.265139	21.005696
68.071479	2357.446895	21.010714
68.281281	2372.036601	21.015731
68.501902	2364.811679	21.020749
68.300246	2361.921911	21.025767
68.416591	2366.582270	21.030784
68.209670	2370.075093	21.035802
68.604646	2362.340694	21.040819
68.957604	2369.302887	21.045837
68.625881	2359.951918	21.050855
68.686668	2352.607758	21.055872
68.840743	2370.604794	21.060890
68.817792	2381.670883	21.065907
69.000374	2390.290430	21.070925
68.797894	2393.114078	21.075943
69.190615	2385.449916	21.080960
69.234543	2386.422963	21.085978
69.280030	2380.726647	21.090995
69.454172	2389.214529	21.096013
69.400646	2387.268895	21.101031
69.712866	2387.689383	21.106048
69.775124	2384.656599	21.111066
69.788180	2401.620571	21.116083
69.767968	2403.590944	21.121101
69.617088	2415.324796	21.126119
70.096749	2408.965435	21.131136
70.107233	2411.642290	21.136154
70.231449	2409.003952	21.141171
70.268918	2392.009139	21.146189
70.365152	2413.424348	21.151207
70.478437	2416.820964	21.156224
70.469394	2405.856934	21.161242
70.294066	2403.269081	21.166259
70.614920	2397.628821	21.171277
70.600846	2405.292573	21.176295
70.828305	2395.209271	21.181312
70.636807	2394.469602	21.186330
70.896218	2396.588042	21.191347
70.828824	2386.462730	21.196365
70.651773	2397.332858	21.201383
70.669036	2386.547549	21.206400
71.000988	2399.343235	21.211418
70.540052	2421.309345	21.216435
71.022653	2430.598960	21.221453
71.139905	2426.070788	21.226471
71.104985	2435.812037	21.231488
71.430256	2428.265094	21.236506
71.122476	2436.544474	21.241523
71.394841	2448.066295	21.246541
71.635100	2460.700427	21.251559
71.567712	2464.604036	21.256576
71.886399	2460.813370	21.261594
71.663762	2453.657521	21.266611
71.863567	2455.328376	21.271629
71.696684	2464.985947	21.276647
71.986843	2449.069696	21.281664
71.890712	2462.228275	21.286682
72.056245	2474.672027	21.291699
72.350447	2469.380803	21.296717
72.290470	2481.992327	21.301735
72.406435	2478.299521	21.306752
72.725793	2480.195288	21.311770
72.592659	2476.520813	21.316787
72.604785	2473.360677	21.321805
72.803702	2476.059157	21.326823
72.875107	2478.310242	21.331840
73.077244	2479.639797	21.336858
72.898686	2477.475856	21.341875
73.152798	2477.417013	21.346893
72.786288	2480.883481	21.351911
72.786874	2471.281285	21.356928
73.137351	2474.200566	21.361946
72.801515	2487.178520	21.366963
72.754742	2476.435815	21.371981
72.895382	2491.346290	21.376999
73.259250	2502.688281	21.382016
73.296556	2498.860645	21.387034
73.323026	2513.686276	21.392051
73.612390	2509.825450	21.397069
73.269021	2502.313968	21.402087
73.417381	2533.760881	21.407104
73.877304	2544.883109	21.412122
73.862784	2539.346246	21.417139
74.029694	2536.148513	21.422157
74.144681	2541.116998	21.427175
73.885839	2528.357687	21.432192
74.211217	2529.430876	21.437210
74.051450	2535.003184	21.442227
74.402950	2553.124096	21.447245
74.575445	2561.563923	21.452263
74.480869	2564.388077	21.457280
74.868940	2562.194265	21.462298
74.691996	2573.214093	21.467315
74.986308	2556.754959	21.472333
74.814848	2557.232547	21.477351
74.906728	2557.494585	21.482368
75.239976	2554.780345	21.487386
74.992549	2558.540908	21.492403
75.119994	2549.260982	21.497421
75.293552	2556.888488	21.502439
75.190616	2554.990759	21.507456
75.632752	2540.909788	21.512474
75.392973	2551.902783	21.517491
75.592071	2563.104540	21.522509
75.873667	2568.148250	21.527527
75.863993	2562.606248	21.532544
76.013444	2578.526298	21.537562
75.752740	2576.719987	21.542579
75.965207	2573.089552	21.547597
76.105821	2575.920116	21.552615
75.905124	2572.520542	21.557632
75.986623	2565.860405	21.562650
75.850118	2573.989714	21.567667
76.106651	2568.994816	21.572685
76.175680	2564.480478	21.577703
75.998230	2579.135554	21.582720
76.153362	2594.106327	21.587738
76.325570	2605.216305	21.592755
76.580371	2597.422873	21.597773
76.544600	2601.112843	21.602791
76.398003	2602.998622	21.607808
76.581853	2615.931158	21.612826
76.536120	2631.047159	21.617843
76.900952	2618.128614	21.622861
77.173510	2628.415786	21.627879
77.073121	2631.909959	21.632896
77.269702	2617.737813	21.637914
77.225491	2622.253533	21.642931
77.659364	2627.079594	21.647949
77.812270	2624.846292	21.652967
77.593331	2623.241326	21.657984
77.775704	2619.750489	21.663002
77.624708	2624.152369	21.668019
78.048309	2643.426154	21.673037
78.526839	2635.149504	21.678055
78.016115	2617.828327	21.683072
78.272733	2621.163511	21.688090
77.906181	2617.019540	21.693107
77.963942	2601.822785	21.698125
78.501700	2634.289532	21.703143
78.709767	2638.130148	21.708160
78.552956	2614.650727	21.713178
78.212761	2631.028686	21.718195
78.284564	2632.521514	21.723213
78.464446	2634.081713	21.728231
78.666419	2634.711556	21.733248
78.942000	2635.797115	21.738266
78.551060	2634.943747	21.743283
78.610295	2645.747840	21.748301
79.141254	2640.824296	21.753319
79.010403	2646.126726	21.758336
79.371049	2660.774844	21.763354
79.336869	2658.386246	21.768371
79.363176	2660.059812	21.773389
79.385466	2665.108218	21.778407
79.325079	2655.847654	21.783424
79.239270	2664.366439	21.788442
79.499249	2661.176527	21.793459
79.547811	2659.759621	21.798477
79.370484	2682.997254	21.803495
79.817634	2693.237312	21.808512
79.945319	2689.661803	21.813530
79.800771	2694.179558	21.818547
79.987117	2694.721243	21.823565
80.171228	2689.718001	21.828583
79.957045	2691.909821	21.833600
80.367136	2688.912210	21.838618
80.502620	2705.901557	21.843635
80.586824	2708.546008	21.848653
80.828702	2698.009566	21.853671
81.042379	2710.422917	21.858688
80.770503	2701.601971	21.863706
80.887878	2705.193238	21.868723
80.720208	2699.121426	21.873741
80.835247	2703.859263	21.878759
81.002755	2714.440604	21.883776
81.123844	2703.631028	21.888794
80.975549	2707.125852	21.893811
81.423865	2724.699311	21.898829
81.674941	2739.949431	21.903847
81.391981	2744.412519	21.908864
81.305437	2737.454507	21.913882
81.427891	2735.264015	21.918899
81.431241	2739.021564	21.923917
81.550200	2740.850683	21.928935
81.676993	2746.603454	21.933952
81.941690	2757.646491	21.938970
81.833070	2766.589548	21.943987
81.928822	2764.340476	21.949005
82.276951	2760.635615	21.954023
82.167993	2770.249161	21.959040
82.189819	2766.431300	21.964058
82.162747	2786.132667	21.969075
82.555130	2790.829818	21.974093
82.932724	2789.862828	21.979111
82.568622	2794.114943	21.984128
82.922217	2785.002414	21.989146
82.694365	2794.020305	21.994163
82.842250	2807.378604	21.999181
83.062821	2776.807862	22.004199
82.861998	2788.740788	22.009216
82.983611	2788.624711	22.014234
83.479911	2804.490632	22.019251
83.130091	2813.900320	22.024269
83.454882	2809.988687	22.029287
83.313997	2812.620944	22.034304
83.896882	2804.338573	22.039322
83.778224	2818.437736	22.044339
83.877959	2812.389010	22.049357
84.245011	2810.648217	22.054375
83.845625	2805.505546	22.059392
84.099187	2801.839135	22.064410
83.969250	2803.357443	22.069427
83.943145	2796.547676	22.074445
84.603245	2795.543451	22.079463
84.151002	2802.210381	22.084480
84.653546	2805.909077	22.089498
84.531827	2794.337444	22.094515
84.440924	2810.252375	22.099533
84.632488	2822.995239	22.104551
84.584041	2821.164058	22.109568
84.720655	2827.513627	22.114586
84.907161	2828.459599	22.119603
84.904521	2828.529792	22.124621
84.849928	2831.224560	22.129639
84.949285	2838.671171	22.134656
85.243317	2846.113175	22.139674
85.193818	2853.212759	22.144691
85.336237	2859.541304	22.149709
85.641280	2844.877235	22.154727
85.710469	2864.054162	22.159744
85.569396	2849.261851	22.164762
85.559972	2854.507675	22.169779
85.798791	2870.471720	22.174797
86.004942	2879.301808	22.179815
85.885936	2879.249899	22.184832
86.144522	2876.432595	22.189850
86.145440	2878.928838	22.194867
86.235466	2893.014450	22.199885
86.345200	2873.094726	22.204903
86.132698	2879.905134	22.209920
86.014460	2891.132798	22.214938
86.335163	2898.686949	22.219955
86.424237	2904.644820	22.224973
86.803135	2900.437625	22.229991
86.614401	2913.350486	22.235008
87.234324	2918.680120	22.240026
87.542632	2920.929523	22.245043
87.800124	2914.029141	22.250061
87.777715	2899.704155	22.255079
87.468367	2886.065539	22.260096
87.421835	2892.977260	22.265114
87.579472	2888.214929	22.270131
87.557050	2893.851082	22.275149
87.890145	2907.680018	22.280167
87.928934	2933.196758	22.285184
88.050436	2921.289971	22.290202
88.217991	2917.454685	22.295219
88.077986	2928.639125	22.300237
88.262089	2915.524029	22.305255
88.016355	2921.156544	22.310272
88.176556	2923.997321	22.315290
87.840791	2921.190038	22.320307
87.973263	2923.290947	22.325325
88.522680	2941.174505	22.330343
88.546343	2945.581470	22.335360
88.779149	2939.714238	22.340378
88.667048	2952.807767	22.345395
88.370218	2948.276809	22.350413
88.691518	2938.501450	22.355431
88.633300	2952.908842	22.360448
88.863061	2962.503935	22.365466
89.075155	2968.238363	22.370483
88.946935	2974.806157	22.375501
89.219271	2972.218441	22.380519
89.145630	2983.033704	22.385536
89.402192	2987.596674	22.390554
89.565029	2997.771325	22.395571
89.514262	3012.055892	22.400589
89.430002	3000.990882	22.405607
89.446331	3009.012687	22.410624
89.971569	3021.263982	22.415642
90.199055	3018.674616	22.420659
89.869235	3020.253926	22.425677
90.260039	3027.054464	22.430695
90.390846	3031.839400	22.435712
90.368238	3038.075609	22.440730
90.537045	3024.531078	22.445747
90.526687	3034.060781	22.450765
90.925769	3044.273585	22.455783
91.015745	3047.592110	22.460800
90.902070	3048.073942	22.465818
91.324398	3052.260343	22.470835
91.331423	3056.351205	22.475853
91.650867	3046.205630	22.480871
91.328249	3044.686646	22.485888
91.623327	3042.424280	22.490906
91.740890	3040.319195	22.495923
91.003361	3051.669388	22.500941
91.364882	3039.188227	22.505959
91.304019	3052.815868	22.510976
91.486537	3068.429989	22.515994
91.725104	3065.964763	22.521011
91.793190	3074.693373	22.526029
92.011299	3061.588281	22.531047
92.188061	3084.329835	22.536064
92.045108	3086.415258	22.541082
92.610241	3086.251479	22.546099
92.669226	3087.072875	22.551117
92.866149	3087.085291	22.556135
92.902716	3083.108624	22.561152
93.084631	3090.864536	22.566170
93.611562	3086.688732	22.571187
93.100854	3102.136349	22.576205
93.129514	3096.580340	22.581223
93.280229	3092.264349	22.586240
93.333859	3085.565682	22.591258
93.409820	3075.503234	22.596275
93.377193	3088.943179	22.601293
93.356011	3078.819619	22.606311
93.533911	3086.278567	22.611328
93.609413	3082.654506	22.616346
93.718473	3089.127629	22.621363
93.332444	3114.760929	22.626381
93.684216	3110.199907	22.631399
93.980167	3120.022339	22.636416
93.487727	3116.883050	22.641434
94.207363	3145.538293	22.646451
94.014250	3154.066024	22.651469
94.137754	3142.322510	22.656487
94.274312	3152.916944	22.661504
94.381190	3168.120452	22.666522
94.792884	3174.552656	22.671539
94.680935	3176.401874	22.676557
94.836720	3171.585829	22.681575
94.857401	3175.566202	22.686592
94.832737	3169.921345	22.691610
95.328087	3164.307878	22.696627
95.285501	3171.777318	22.701645
95.451892	3174.023833	22.706663
95.625292	3185.751924	22.711680
95.510269	3201.193307	22.716698
96.039783	3181.468772	22.721715
95.867629	3188.708065	22.726733
96.298770	3192.323776	22.731751
96.302219	3175.828982	22.736768
96.117630	3182.286104	22.741786
96.132812	3189.175161	22.746803
95.968252	3183.791990	22.751821
96.058188	3174.093691	22.756839
96.490031	3182.388250	22.761856
96.117686	3180.421186	22.766874
96.797263	3178.854293	22.771891
96.529632	3195.311010	22.776909
96.582819	3193.752350	22.781927
96.914616	3201.597721	22.786944
96.983190	3199.060174	22.791962
97.337309	3207.546718	22.796979
96.965289	3209.869216	22.801997
97.332011	3200.853485	22.807015
97.400807	3211.540649	22.812032
97.312255	3214.313140	22.817050
97.548159	3219.883497	22.822067
97.433058	3225.070140	22.827085
97.718256	3238.272661	22.832103
97.811265	3237.001896	22.837120
97.718333	3233.168239	22.842138
97.875330	3218.862129	22.847155
97.595342	3246.220979	22.852173
98.286784	3248.064217	22.857191
98.393127	3258.498367	22.862208
98.303229	3269.050775	22.867226
98.297916	3251.793198	22.872243
98.080962	3279.845213	22.877261
98.726610	3271.628601	22.882279
99.165540	3291.689814	22.887296
99.279817	3291.698959	22.892314
99.495036	3283.945188	22.897331
99.754916	3281.430738	22.902349
99.608371	3282.408546	22.907367
99.560426	3282.202377	22.912384
99.605710	3288.471561	22.917402
99.419779	3280.684870	22.922419
99.265912	3279.833625	22.927437
99.531511	3283.171604	22.932455
99.878477	3277.136961	22.937472
99.812018	3294.452640	22.942490
99.701807	3301.960482	22.947507
99.922864	3309.769878	22.952525
100.042860	3298.243749	22.957543
100.186744	3318.804134	22.962560
99.976981	3327.342585	22.967578
100.690597	3324.001596	22.972595
100.824518	3325.198014	22.977613
100.449411	3341.439974	22.982631
100.838323	3336.307016	22.987648
100.754828	3344.974608	22.992666
100.807887	3327.497463	22.997683
100.903989	3340.848246	23.002701
100.954919	3354.038792	23.007719
100.953087	3349.853446	23.012736
101.144045	3365.140102	23.017754
101.324344	3356.214141	23.022771
101.473928	3372.766666	23.027789
101.514075	3386.979864	23.032807
102.048812	3377.079594	23.037824
101.812474	3386.313398	23.042842
102.050767	3380.456906	23.047859
102.206775	3389.829811	23.052877
102.354452	3393.799098	23.057895
102.233415	3375.429428	23.062912
102.125227	3387.526243	23.067930
102.393651	3402.545810	23.072947
102.476983	3416.100732	23.077965
102.518672	3411.863690	23.082983
102.611973	3413.984132	23.088000
102.237365	3420.209371	23.093018
102.640029	3421.368081	23.098035
103.227973	3435.514032	23.103053
103.842802	3440.837606	23.108071
103.469317	3438.817153	23.113088
102.919621	3434.638853	23.118106
103.495491	3431.183598	23.123123
103.493130	3439.605951	23.128141
103.542227	3441.535279	23.133159
103.968471	3453.239115	23.138176
104.205054	3457.156326	23.143194
104.114529	3457.008371	23.148211
104.138764	3467.731028	23.153229
104.308453	3466.271593	23.158247
104.642602	3449.358088	23.163264
104.094375	3462.093019	23.168282
104.367418	3462.620407	23.173299
104.576853	3469.381822	23.178317
104.702855	3486.091512	23.183335
104.745186	3483.755103	23.188352
105.106847	3486.422539	23.193370
105.099657	3484.771073	23.198387
105.257773	3478.511657	23.203405
105.224082	3479.997985	23.208423
105.506061	3494.589424	23.213440
105.521736	3516.367695	23.218458
105.537957	3510.835247	23.223475
105.873638	3522.076548	23.228493
105.759486	3517.680586	23.233511
105.723156	3519.496483	23.238528
105.580587	3533.268755	23.243546
106.074181	3531.321937	23.248563
106.033609	3547.382456	23.253581
105.872245	3554.372107	23.258599
106.306141	3555.447716	23.263616
106.274214	3576.758352	23.268634
106.827554	3563.103748	23.273651
107.142820	3577.201581	23.278669
107.112664	3575.406264	23.283687
107.103703	3566.546102	23.288704
107.217281	3578.951298	23.293722
107.273677	3572.694086	23.298739
107.400993	3566.357442	23.303757
107.496072	3561.319814	23.308775
107.692553	3567.931840	23.313792
107.419782	3594.065319	23.318810
107.814839	3588.260402	23.323827
107.899267	3595.373628	23.328845
107.814085	3595.742108	23.333863
107.855748	3591.546754	23.338880
107.794947	3594.063547	23.343898
108.080863	3617.853586	23.348915
108.112593	3632.537294	23.353933
108.226549	3629.372104	23.358951
108.511828	3630.195900	23.363968
108.713791	3639.672386	23.368986
108.980171	3640.572927	23.374003
109.200741	3650.256974	23.379021
109.300498	3651.694889	23.384039
109.314072	3642.673086	23.389056
109.241411	3649.119779	23.394074
109.339451	3640.554096	23.399091
109.881627	3637.129956	23.404109
109.531371	3642.970946	23.409127
109.662333	3637.493114	23.414144
109.610049	3638.751034	23.419162
109.466738	3637.847238	23.424179
109.836209	3657.255447	23.429197
109.971353	3671.130376	23.434215
110.156683	3670.072272	23.439232
110.097265	3670.172324	23.444250
110.094008	3664.157215	23.449267
110.421419	3660.979974	23.454285
110.444726	3693.532778	23.459303
110.789370	3700.621557	23.464320
110.994739	3693.613697	23.469338
111.108090	3700.780853	23.474355
111.214438	3688.246457	23.479373
111.395331	3688.008375	23.484391
111.604556	3681.381772	23.489408
111.692806	3691.160937	23.494426
111.385415	3685.976782	23.499443
111.730235	3695.674578	23.504461
111.550091	3717.868953	23.509479
112.081238	3709.945050	23.514496
112.223300	3720.838569	23.519514
111.923848	3723.089307	23.524531
112.240415	3724.061481	23.529549
112.054543	3722.863925	23.534567
112.131449	3733.239480	23.539584
112.117256	3732.466310	23.544602
112.230292	3739.953222	23.549619
112.454942	3748.088624	23.554637
112.499674	3760.464397	23.559655
112.764465	3767.770734	23.564672
112.884889	3780.019054	23.569690
112.687014	3778.659303	23.574707
113.212177	3788.583657	23.579725
113.076355	3798.505035	23.584743
113.162985	3800.211670	23.589760
113.270809	3809.851454	23.594778
113.513892	3827.555556	23.599795
113.752554	3816.536210	23.604813
113.927023	3819.336213	23.609831
114.187615	3824.711763	23.614848
114.346477	3823.715898	23.619866
114.678512	3838.913174	23.624883
114.868387	3838.794079	23.629901
114.712937	3836.809985	23.634919
115.393687	3829.910914	23.639936
115.144662	3838.556133	23.644954
115.129446	3835.821697	23.649971
115.650397	3836.024275	23.654989
115.378980	3841.738137	23.660007
115.523452	3834.307203	23.665024
115.102319	3839.981630	23.670042
115.046934	3840.031803	23.675059
115.449040	3829.637807	23.680077
115.575177	3853.337286	23.685095
115.871294	3866.797598	23.690112
115.772589	3857.972965	23.695130
115.755585	3877.252791	23.700147
115.947482	3880.773159	23.705165
115.886582	3893.168068	23.710183
116.269162	3894.971087	23.715200
116.221894	3905.539324	23.720218
116.166453	3912.215173	23.725235
116.395642	3923.055066	23.730253
116.393328	3939.224630	23.735271
116.825225	3922.787381	23.740288
116.984718	3934.241168	23.745306
117.158076	3941.122138	23.750323
117.034687	3950.071860	23.755341
117.168522	3967.375271	23.760359
117.716879	3955.579838	23.765376
117.532821	3951.784289	23.770394
117.266167	3961.765579	23.775411
117.780348	3972.235969	23.780429
118.137718	3979.213717	23.785447
118.143474	3983.475509	23.790464
118.449260	3986.918814	23.795482
117.933256	3986.186031	23.800499
118.527873	3989.346173	23.805517
118.593537	4006.549473	23.810535
118.633316	4013.030100	23.815552
119.019127	4011.382537	23.820570
118.863589	4006.655080	23.825587
119.325828	4007.916988	23.830605
119.093003	4014.663530	23.835623
119.052410	3999.322011	23.840640
119.149080	4022.198650	23.845658
119.762758	4039.088199	23.850675
119.805767	4036.048431	23.855693
119.633284	4037.208920	23.860711
120.002834	4035.790424	23.865728
120.109630	4031.519227	23.870746
119.958797	4057.474670	23.875763
120.275582	4059.736228	23.880781
120.524482	4062.896818	23.885799
120.544794	4056.752070	23.890816
120.649624	4062.321555	23.895834
120.772560	4061.358384	23.900851
120.916141	4076.025604	23.905869
120.790174	4098.450550	23.910887
120.934587	4089.200958	23.915904
121.333290	4090.206043	23.920922
120.820272	4099.135978	23.925939
121.347718	4099.576470	23.930957
121.383511	4115.129275	23.935975
121.462383	4124.448047	23.940992
121.794579	4116.767056	23.946010
121.958508	4133.633778	23.951027
122.276046	4141.940264	23.956045
122.250945	4154.978695	23.961063
122.410699	4150.250277	23.966080
122.924806	4139.954501	23.971098
122.885810	4152.187330	23.976115
123.016564	4138.744183	23.981133
122.761038	4144.935857	23.986151
122.956505	4147.685598	23.991168
123.288615	4142.373570	23.996186
123.018233	4150.330740	24.001203
123.726404	4158.898679	24.006221
123.418907	4165.647389	24.011239
123.644137	4162.555832	24.016256
124.040716	4159.129654	24.021274
123.657981	4170.098002	24.026291
123.704053	4159.069292	24.031309
123.707131	4181.589573	24.036327
123.875727	4184.686290	24.041344
124.030528	4200.706931	24.046362
123.808762	4200.901137	24.051379
124.714115	4204.463929	24.056397
124.513839	4231.451878	24.061415
124.851407	4226.651141	24.066432
124.673943	4222.744590	24.071450
124.899213	4227.412316	24.076467
125.071356	4221.307770	24.081485
125.007812	4240.099263	24.086503
125.242958	4257.248456	24.091520
125.190719	4252.847567	24.096538
125.345368	4255.697382	24.101555
125.748784	4259.470691	24.106573
125.635361	4274.692788	24.111591
125.756686	4285.112554	24.116608
126.514791	4274.045637	24.121626
126.215229	4271.957343	24.126643
126.569794	4257.362900	24.131661
126.816796	4281.445436	24.136679
127.047354	4281.136932	24.141696
127.340583	4282.091347	24.146714
127.386964	4276.339068	24.151731
127.596385	4263.700166	24.156749
127.488481	4257.792280	24.161767
127.424289	4261.926725	24.166784
127.814690	4253.354523	24.171802
127.787085	4275.452831	24.176819
127.667094	4276.050707	24.181837
127.839787	4280.925569	24.186855
127.867647	4274.673972	24.191872
128.120005	4272.452745	24.196890
128.074910	4282.277152	24.201907
128.088780	4293.392657	24.206925
128.314542	4307.055929	24.211943
128.335617	4309.489227	24.216960
128.646465	4306.248844	24.221978
128.333822	4317.432492	24.226995
128.385954	4328.018451	24.232013
128.713794	4341.636932	24.237031
128.983777	4343.987765	24.242048
129.150860	4358.003311	24.247066
129.479760	4381.187394	24.252083
129.340165	4363.618080	24.257101
129.651833	4376.690817	24.262119
129.589533	4398.539903	24.267136
129.833091	4385.562964	24.272154
130.037299	4394.867881	24.277171
130.504583	4402.574935	24.282189
130.541010	4394.353285	24.287207
130.438105	4411.027776	24.292224
130.862152	4411.165666	24.297242
130.829346	4422.634266	24.302259
131.016806	4424.924729	24.307277
131.474299	4420.025373	24.312295
131.053437	4415.654245	24.317312
131.559033	4431.219110	24.322330
131.261188	4428.428905	24.327347
131.685976	4441.809003	24.332365
131.687710	4455.356661	24.337383
131.662263	4458.068154	24.342400
131.809762	4447.824486	24.347418
131.730061	4466.838224	24.352435
131.870133	4473.114273	24.357453
132.078005	4471.288183	24.362471
132.183362	4489.633544	24.367488
132.738979	4489.889071	24.372506
132.788164	4510.367858	24.377523
132.777664	4518.038164	24.382541
133.139771	4510.547718	24.387559
133.035831	4509.798395	24.392576
133.749831	4514.227175	24.397594
133.126848	4511.473749	24.402611
133.505193	4517.039937	24.407629
133.148964	4519.889175	24.412647
132.954386	4537.113228	24.417664
133.846114	4532.831884	24.422682
133.687515	4552.029637	24.427699
133.585401	4561.597486	24.432717
133.925656	4571.101300	24.437735
134.148964	4582.432810	24.442752
134.639440	4588.846685	24.447770
134.220790	4599.144458	24.452787
134.012913	4600.293512	24.457805
134.589799	4602.800771	24.462823
134.769406	4621.145436	24.467840
135.214008	4621.431910	24.472858
134.971730	4623.002028	24.477875
135.353840	4642.017234	24.482893
135.635448	4637.623280	24.487911
135.815268	4634.902148	24.492928
136.045927	4652.492701	24.497946
135.957452	4645.543207	24.502963
136.245002	4654.486456	24.507981
136.654652	4674.386574	24.512999
136.572337	4669.272383	24.518016
136.971504	4663.885709	24.523034
136.917616	4669.795831	24.528051
137.382203	4661.672594	24.533069
137.645480	4656.493428	24.538087
137.527829	4659.918265	24.543104
137.565801	4657.177652	24.548122
137.543277	4655.936887	24.553139
137.407385	4648.543231	24.558157
137.946826	4665.037046	24.563175
138.062236	4679.167725	24.568192
138.450980	4677.451891	24.573210
138.240315	4688.083093	24.578227
138.186715	4689.088150	24.583245
138.242052	4675.195951	24.588263
138.206573	4681.616453	24.593280
138.569588	4698.299702	24.598298
138.692877	4715.334017	24.603315
138.771068	4715.803880	24.608333
139.009586	4709.364535	24.613351
139.214344	4723.758855	24.618368
139.298788	4724.648578	24.623386
139.011578	4733.808113	24.628403
139.242126	4751.892530	24.633421
139.900822	4762.282094	24.638439
139.822086	4782.541414	24.643456
140.085005	4779.665178	24.648474
140.124242	4784.423265	24.653491
139.844826	4791.187683	24.658509
140.279254	4807.707270	24.663527
140.500943	4807.780959	24.668544
140.746110	4802.123208	24.673562
140.836066	4818.918245	24.678579
140.927103	4818.914696	24.683597
141.370366	4824.766746	24.688615
140.989151	4829.382890	24.693632
141.422808	4830.799209	24.698650
141.453498	4845.953559	24.703667
141.168109	4866.232960	24.708685
141.626197	4854.728956	24.713703
141.833662	4875.558867	24.718720
142.125097	4889.003516	24.723738
141.996189	4882.831126	24.728755
142.114548	4900.795661	24.733773
142.804196	4897.497291	24.738791
142.649292	4906.137389	24.743808
143.236777	4900.609667	24.748826
143.109281	4909.370051	24.753843
143.236351	4912.701747	24.758861
143.801072	4905.602862	24.763879
143.779132	4916.722365	24.768896
143.765783	4893.919780	24.773914
143.641307	4903.371839	24.778931
143.770603	4907.160286	24.783949
144.127575	4911.155620	24.788967
143.926691	4927.063722	24.793984
143.969878	4938.923325	24.799002
144.150627	4929.224284	24.804019
144.075020	4937.718216	24.809037
144.337160	4947.363525	24.814055
144.217585	4959.281142	24.819072
144.654120	4975.659210	24.824090
144.978300	4991.362103	24.829107
144.991558	5000.215825	24.834125
145.185687	5002.481255	24.839143
145.289581	5010.449069	24.844160
145.753624	5011.004409	24.849178
145.882189	5012.870798	24.854195
145.731793	5019.143484	24.859213
146.160553	5020.976020	24.864231
146.512985	5035.849025	24.869248
146.494960	5036.886811	24.874266
146.335549	5026.816323	24.879283
146.698887	5032.824190	24.884301
146.706509	5048.941683	24.889319
146.754234	5054.405597	24.894336
146.811473	5062.689834	24.899354
147.258832	5077.517663	24.904371
147.492104	5080.322353	24.909389
147.810562	5094.490336	24.914407
147.811058	5097.148437	24.919424
148.111143	5089.525826	24.924442
148.138411	5097.899293	24.929459
147.839611	5113.586341	24.934477
148.173587	5117.489064	24.939495
148.615060	5122.889120	24.944512
148.775457	5128.712823	24.949530
148.891072	5148.927905	24.954547
148.779644	5156.317143	24.959565
148.917704	5158.323332	24.964583
148.715113	5164.681479	24.969600
149.222468	5176.865390	24.974618
149.263855	5185.870095	24.979635
149.423623	5190.573741	24.984653
149.513658	5198.160046	24.989671
149.716555	5216.511013	24.994688
150.096041	5210.192278	24.999706
150.293213	5227.963441	25.004723
150.144046	5244.496057	25.009741
150.616445	5249.486284	25.014759
150.700842	5251.893123	25.019776
150.878315	5261.371103	25.024794
151.188468	5271.535503	25.029811
151.080949	5275.712023	25.034829
151.292289	5271.699226	25.039847
151.001735	5289.406546	25.044864
151.286288	5291.280662	25.049882
151.841413	5301.477051	25.054899
151.831201	5312.858311	25.059917
152.019708	5326.525877	25.064935
152.258741	5336.410309	25.069952
152.263630	5332.891499	25.074970
152.329851	5337.464175	25.079987
152.487386	5341.404771	25.085005
152.826952	5353.609064	25.090023
152.894674	5364.046677	25.095040
153.277474	5361.654517	25.100058
153.493669	5361.299939	25.105075
153.572057	5372.174818	25.110093
154.059833	5353.562437	25.115111
153.895046	5354.020495	25.120128
154.059596	5381.008025	25.125146
154.097341	5384.521529	25.130163
153.987301	5394.431783	25.135181
154.217600	5381.327458	25.140199
154.495585	5400.662009	25.145216
154.340398	5420.725710	25.150234
154.837597	5407.947774	25.155251
154.857801	5413.142709	25.160269
154.905708	5405.247800	25.165287
155.363405	5434.450220	25.170304
155.263128	5438.981926	25.175322
155.601115	5430.604773	25.180339
155.286880	5446.837283	25.185357
155.964776	5441.638961	25.190375
156.044395	5456.555478	25.195392
156.477749	5459.286620	25.200410
156.623265	5451.282243	25.205427
156.140867	5453.554396	25.210445
156.793444	5479.061302	25.215463
156.706472	5487.690889	25.220480
156.777648	5482.683367	25.225498
157.231301	5490.412118	25.230515
157.160640	5516.139781	25.235533
157.546828	5506.235947	25.240551
157.785277	5522.283106	25.245568
157.605751	5510.755225	25.250586
157.908251	5525.672779	25.255603
158.090567	5545.858453	25.260621
158.127524	5540.032849	25.265639
157.990739	5547.849739	25.270656
158.462873	5574.341453	25.275674
158.452504	5574.470422	25.280691
158.372941	5582.406630	25.285709
158.595719	5600.655145	25.290727
158.939363	5614.678871	25.295744
159.260258	5630.296721	25.300762
159.524281	5641.434456	25.305779
159.470351	5652.344781	25.310797
159.599825	5649.977505	25.315815
159.659780	5670.752133	25.320832
159.756898	5669.051700	25.325850
160.167613	5680.884212	25.330867
160.433709	5706.278950	25.335885
160.569834	5687.931785	25.340903
160.823864	5698.891663	25.345920
160.916183	5721.382487	25.350938
161.389802	5721.219254	25.355955
161.400471	5732.562718	25.360973
161.630836	5731.662808	25.365991
161.789417	5734.831185	25.371008
161.632432	5747.873837	25.376026
161.852404	5759.370162	25.381043
161.881570	5748.912096	25.386061
162.498246	5761.180383	25.391079
162.592295	5764.293278	25.396096
162.361473	5785.631132	25.401114
162.945719	5786.232400	25.406131
162.937696	5793.819054	25.411149
163.377652	5783.543515	25.416167
163.354383	5793.800755	25.421184
163.341422	5805.517123	25.426202
163.546901	5810.726463	25.431219
163.646005	5811.128330	25.436237
164.028977	5814.895558	25.441255
164.125830	5816.793271	25.446272
163.793157	5813.698684	25.451290
164.345576	5828.375993	25.456307
164.082778	5843.895593	25.461325
164.544024	5844.617201	25.466343
164.585893	5862.313946	25.471360
164.438446	5868.881405	25.476378
165.054450	5878.673180	25.481395
165.036478	5895.108808	25.486413
165.755644	5901.494499	25.491431
165.576708	5903.900062	25.496448
165.652296	5907.854342	25.501466
166.273136	5908.250329	25.506483
165.942968	5928.804287	25.511501
166.575099	5919.595092	25.516519
166.605555	5911.811489	25.521536
166.662345	5916.478819	25.526554
166.976215	5924.248208	25.531571
167.143276	5939.313751	25.536589
167.156898	5941.555594	25.541607
167.647639	5942.449918	25.546624
167.382918	5938.531758	25.551642
167.482784	5966.669730	25.556659
167.437883	5969.003936	25.561677
167.544637	5972.979858	25.566695
167.837824	5992.620154	25.571712
168.020918	6007.814235	25.576730
168.324990	6010.003371	25.581747
168.356450	6033.098879	25.586765
168.529259	6038.820856	25.591783
168.899098	6047.342194	25.596800
169.033888	6065.978681	25.601818
169.462738	6065.532250	25.606835
169.324800	6063.750124	25.611853
169.898126	6083.328495	25.616871
170.225602	6084.698298	25.621888
170.524115	6079.516781	25.626906
170.502691	6079.475508	25.631923
170.801762	6075.683874	25.636941
171.117329	6079.138633	25.641959
170.875003	6070.008083	25.646976
170.915477	6081.203152	25.651994
171.186480	6111.800095	25.657011
171.060577	6118.435369	25.662029
171.451923	6113.053435	25.667047
171.564056	6122.609674	25.672064
171.563849	6141.337071	25.677082
171.763743	6127.730376	25.682100
171.645615	6148.123187	25.687117
171.870266	6173.138069	25.692135
171.995383	6176.110066	25.697152
172.164195	6199.384336	25.702170
172.454217	6211.382492	25.707188
172.792628	6211.194347	25.712205
172.963846	6238.166502	25.717223
173.598407	6236.967064	25.722240
173.446400	6241.493766	25.727258
173.729807	6237.981891	25.732276
173.511979	6259.560799	25.737293
173.718007	6271.457901	25.742311
174.098770	6259.615200	25.747328
173.921767	6281.744175	25.752346
174.466495	6296.156617	25.757364
174.548705	6294.232560	25.762381
174.679353	6305.906671	25.767399
174.912071	6321.738633	25.772416
174.882778	6334.418095	25.777434
175.084759	6333.297214	25.782452
175.220396	6347.946619	25.787469
175.508249	6360.685529	25.792487
175.596229	6350.818233	25.797504
175.852404	6371.174687	25.802522
176.257243	6377.765689	25.807540
176.580604	6383.154202	25.812557
176.367034	6387.103617	25.817575
176.421403	6386.504845	25.822592
176.587331	6405.856398	25.827610
177.019964	6416.466347	25.832628
177.220338	6421.616096	25.837645
177.063942	6439.172598	25.842663
177.382591	6450.425922	25.847680
177.452409	6451.000390	25.852698
177.700572	6475.519658	25.857716
178.042733	6483.552021	25.862733
178.073442	6483.048509	25.867751
178.466196	6490.083366	25.872768
178.646420	6501.343848	25.877786
178.576640	6508.170048	25.882804
179.110950	6512.213282	25.887821
179.650936	6525.696633	25.892839
180.008060	6519.044398	25.897856
180.064359	6520.311777	25.902874
180.254665	6515.181862	25.907892
180.308159	6512.080423	25.912909
180.500709	6528.132654	25.917927
180.702526	6532.059147	25.922944
180.387525	6545.552267	25.927962
180.585594	6532.014829	25.932980
180.889594	6549.352838	25.937997
180.963703	6571.519483	25.943015
181.267976	6565.939934	25.948032
181.313785	6572.088676	25.953050
181.448549	6590.621834	25.958068
181.791043	6601.194038	25.963085
181.758870	6599.399887	25.968103
182.114302	6613.834449	25.973120
182.077170	6621.949244	25.978138
182.125103	6641.638752	25.983156
182.507188	6647.295659	25.988173
182.589129	6663.343465	25.993191
183.011073	6662.398856	25.998208
183.080639	6679.480413	26.003226
183.436241	6689.191292	26.008244
183.749210	6698.216178	26.013261
183.804270	6697.530650	26.018279
184.131745	6696.709543	26.023296
184.182418	6713.206745	26.028314
184.363168	6720.806758	26.033332
184.827866	6719.736948	26.038349
184.640551	6738.160475	26.043367
184.874266	6743.085880	26.048384
185.177093	6747.687997	26.053402
185.113552	6748.249859	26.058420
185.170628	6769.411530	26.063437
185.616092	6775.779411	26.068455
185.912640	6777.925403	26.073472
185.911758	6794.643062	26.078490
186.375504	6804.918149	26.083508
186.537321	6809.923973	26.088525
186.498535	6806.336838	26.093543
186.956614	6817.058626	26.098560
186.909664	6835.578782	26.103578
187.262504	6829.534332	26.108596
187.540465	6823.773965	26.113613
187.279979	6834.460133	26.118631
187.431270	6831.631505	26.123648
187.337112	6855.116373	26.128666
187.797694	6856.143716	26.133684
187.925330	6873.355287	26.138701
187.958918	6887.010042	26.143719
188.544997	6888.162350	26.148736
188.465981	6905.624681	26.153754
188.608018	6933.738515	26.158772
188.890382	6920.032454	26.163789
189.021190	6934.673753	26.168807
189.209197	6964.010219	26.173824
189.557726	6972.805719	26.178842
189.632675	6975.829473	26.183860
190.034937	6987.174901	26.188877
189.441994	6994.295671	26.193895
190.291620	7017.549233	26.198912
190.350227	7026.977042	26.203930
190.757996	7041.473444	26.208948
191.111541	7050.176801	26.213965
190.947798	7057.616529	26.218983
191.003433	7069.791895	26.224000
191.341000	7077.325216	26.229018
191.289382	7094.295722	26.234036
191.874666	7107.046738	26.239053
191.838665	7108.497168	26.244071
192.490731	7125.578259	26.249088
192.875797	7135.692510	26.254106
192.736273	7138.360309	26.259124
193.421290	7136.010493	26.264141
193.082526	7153.387641	26.269159
193.980047	7161.406561	26.274176
194.265296	7168.883202	26.279194
194.092378	7154.144048	26.284212
194.954706	7140.629434	26.289229
194.890835	7157.168867	26.294247
195.353389	7141.671827	26.299264
195.181432	7139.363587	26.304282
195.096907	7139.786379	26.309300
195.336822	7139.971272	26.314317
195.664736	7130.535600	26.319335
195.352158	7139.198644	26.324352
195.416664	7153.579389	26.329370
195.600579	7162.150959	26.334388
195.704803	7157.696622	26.339405
195.900412	7191.970346	26.344423
195.817130	7202.162025	26.349440
195.848900	7222.245569	26.354458
196.156776	7240.458698	26.359476
196.511586	7245.187049	26.364493
196.723842	7274.033363	26.369511
196.851350	7274.847993	26.374528
197.091561	7289.751924	26.379546
197.096487	7309.643118	26.384564
197.580702	7314.013024	26.389581
197.659600	7326.224124	26.394599
197.948283	7350.856199	26.399616
198.062907	7351.399670	26.404634
198.420192	7368.187133	26.409652
198.653506	7387.958782	26.414669
198.688074	7393.427653	26.419687
199.227574	7407.265471	26.424704
199.363574	7412.934176	26.429722
199.404472	7423.500061	26.434740
200.044949	7439.987206	26.439757
199.938240	7442.571663	26.444775
200.174546	7445.520804	26.449792
200.420932	7452.673215	26.454810
200.586314	7462.035599	26.459828
200.929361	7467.040830	26.464845
200.897495	7478.506387	26.469863
200.968930	7490.054909	26.474880
201.038636	7496.560780	26.479898
201.233485	7508.209424	26.484916
201.128689	7530.083278	26.489933
201.504411	7540.497833	26.494951
201.706018	7556.276322	26.499968
201.583209	7573.195310	26.504986
201.857771	7593.213218	26.510004
202.167632	7600.134682	26.515021
201.954516	7633.518392	26.520039
202.333853	7639.417119	26.525056
202.887984	7661.276005	26.530074
202.853649	7693.082670	26.535092
203.690931	7699.705956	26.540109
204.044455	7708.482929	26.545127
204.114613	7731.705670	26.550144
204.620097	7734.692300	26.555162
204.769059	7735.256103	26.560180
204.849691	7748.358809	26.565197
204.783319	7771.395451	26.570215
205.528727	7772.285225	26.575232
205.990929	7777.480370	26.580250
205.886281	7793.059239	26.585268
206.129046	7795.972725	26.590285
206.255543	7799.287411	26.595303
206.420623	7796.984030	26.600320
206.604876	7805.382622	26.605338
206.630388	7822.818455	26.610356
206.912683	7824.747207	26.615373
207.068412	7841.242408	26.620391
206.828492	7856.002524	26.625408
207.279121	7855.430375	26.630426
207.421894	7885.171408	26.635444
207.706553	7886.234981	26.640461
207.876931	7911.026885	26.645479
208.160366	7917.616545	26.650496
208.553534	7927.963102	26.655514
208.506711	7952.508993	26.660532
208.707862	7946.801079	26.665549
209.129397	7967.170870	26.670567
209.376075	7971.666059	26.675584
209.738445	7981.746013	26.680602
209.843540	8009.350404	26.685620
210.178258	8013.435675	26.690637
210.440179	8011.920420	26.695655
210.075753	8026.621717	26.700672
210.503055	8034.107592	26.705690
210.367157	8048.979083	26.710708
211.246980	8061.286826	26.715725
211.242657	8084.497974	26.720743
211.282485	8094.932952	26.725760
211.924574	8105.058132	26.730778
211.910362	8108.609577	26.735796
212.279801	8111.658141	26.740813
212.553436	8128.798126	26.745831
212.562531	8142.694300	26.750848
212.762113	8130.750182	26.755866
212.899349	8154.040434	26.760884
213.353819	8164.117890	26.765901
213.272223	8171.583160	26.770919
213.289909	8190.024125	26.775936
213.872595	8190.546999	26.780954
213.437550	8217.725105	26.785972
213.988940	8220.007983	26.790989
213.675140	8242.923154	26.796007
214.001314	8255.654906	26.801024
214.247134	8267.846242	26.806042
214.431041	8291.788231	26.811060
214.940600	8288.967100	26.816077
215.136566	8313.159170	26.821095
215.577898	8331.016765	26.826112
216.168597	8328.031783	26.831130
215.886976	8353.591391	26.836148
216.482172	8354.810048	26.841165
216.309338	8367.526674	26.846183
216.305249	8383.518768	26.851200
216.806886	8390.793260	26.856218
217.121425	8411.744462	26.861236
216.853142	8413.580738	26.866253
217.279774	8431.848085	26.871271
217.285750	8458.292905	26.876288
217.897848	8471.747113	26.881306
217.946780	8488.825372	26.886324
218.339773	8510.330055	26.891341
218.809122	8505.707893	26.896359
219.249129	8521.757500	26.901376
219.416026	8539.870188	26.906394
219.102063	8552.322002	26.911412
219.318556	8553.721394	26.916429
220.021478	8579.168315	26.921447
219.725568	8579.909622	26.926464
220.292640	8597.578188	26.931482
220.387001	8615.754932	26.936500
220.463713	8610.381613	26.941517
220.491026	8646.647535	26.946535
220.874400	8656.232170	26.951552
220.840923	8664.705788	26.956570
221.368417	8691.895799	26.961588
221.810058	8703.723516	26.966605
222.209462	8711.536474	26.971623
222.245829	8731.372274	26.976640
222.364760	8735.632014	26.981658
222.408166	8756.615868	26.986676
222.729845	8773.151571	26.991693
223.019576	8778.064424	26.996711
223.177781	8793.866285	27.001728
223.778398	8795.373153	27.006746
223.892409	8809.484147	27.011764
224.102983	8814.273037	27.016781
224.633272	8819.203655	27.021799
224.276713	8850.518460	27.026816
224.604336	8844.642825	27.031834
224.592184	8863.592028	27.036852
225.158454	8885.055200	27.041869
225.698319	8882.985901	27.046887
225.480473	8919.662365	27.051904
226.032166	8920.269944	27.056922
226.111450	8928.725859	27.061940
226.476670	8951.306950	27.066957
226.354746	8959.036818	27.071975
226.438397	8963.909738	27.076992
226.778764	8983.755488	27.082010
227.099113	9000.403497	27.087028
227.174694	9013.353701	27.092045
227.480670	9033.260332	27.097063
227.732989	9048.888576	27.102080
227.959062	9055.108534	27.107098
227.860012	9078.791271	27.112116
228.353032	9084.806451	27.117133
228.536117	9106.667207	27.122151
228.460461	9130.029512	27.127168
229.137862	9138.643496	27.132186
229.445842	9152.006752	27.137204
229.607563	9158.499679	27.142221
230.205389	9157.723581	27.147239
230.363878	9181.728613	27.152256
230.578969	9180.803078	27.157274
230.665901	9181.666260	27.162292
230.268579	9202.396636	27.167309
230.672311	9214.221547	27.172327
230.821916	9231.569898	27.177344
231.124946	9249.085111	27.182362
231.267430	9267.961985	27.187380
231.234126	9274.414715	27.192397
231.785223	9287.928536	27.197415
232.072386	9315.117578	27.202432
232.765208	9324.337995	27.207450
232.788321	9332.804981	27.212468
233.082876	9348.477741	27.217485
233.480524	9356.119594	27.222503
233.739058	9371.605346	27.227520
234.301451	9368.974584	27.232538
234.377158	9388.923645	27.237556
234.430176	9395.031335	27.242573
234.626916	9397.489565	27.247591
234.988727	9411.215933	27.252608
235.481821	9412.679978	27.257626
235.401867	9420.677250	27.262644
235.787137	9440.055356	27.267661
235.977114	9445.419702	27.272679
236.244647	9445.999424	27.277696
236.396605	9460.109452	27.282714
236.573262	9483.421923	27.287732
236.761991	9478.223575	27.292749
237.003385	9508.830418	27.297767
236.775988	9517.485403	27.302784
237.201592	9536.431609	27.307802
237.190007	9553.085416	27.312820
237.267441	9568.662723	27.317837
237.490767	9575.872683	27.322855
237.666796	9618.817952	27.327872
238.215715	9640.774962	27.332890
238.363496	9653.711396	27.337908
238.522209	9684.893866	27.342925
238.657324	9692.274418	27.347943
238.946382	9714.855000	27.352960
239.380720	9738.141023	27.357978
239.882264	9745.184574	27.362996
239.974560	9781.357273	27.368013
240.713064	9783.686668	27.373031
241.004886	9788.193035	27.378048
242.067963	9788.789418	27.383066
242.443758	9787.260699	27.388084
242.752824	9780.333840	27.393101
242.931599	9779.370162	27.398119
242.936498	9784.939284	27.403136
243.275958	9787.370845	27.408154
243.306917	9778.683730	27.413172
243.203927	9781.019822	27.418189
243.280442	9780.431445	27.423207
243.261279	9792.119493	27.428224
243.455978	9809.023060	27.433242
243.515832	9820.107295	27.438260
243.457711	9827.910539	27.443277
244.118034	9844.608816	27.448295
243.983076	9879.733038	27.453312
244.245680	9888.120577	27.458330
244.499104	9901.635266	27.463348
244.711421	9930.330438	27.468365
245.275026	9939.652124	27.473383
244.826032	9957.665745	27.478400
245.285982	9972.826563	27.483418
245.420198	9991.797037	27.488436
245.496469	10017.128457	27.493453
246.065642	10027.437859	27.498471
245.527206	10055.301007	27.503488
245.846340	10080.394685	27.508506
246.479411	10111.413754	27.513524
246.544063	10135.189170	27.518541
246.839030	10153.308531	27.523559
247.363702	10184.745816	27.528576
247.416289	10189.435978	27.533594
248.056413	10218.402069	27.538612
248.487888	10248.616573	27.543629
249.192678	10253.062719	27.548647
248.941097	10274.224134	27.553664
249.350096	10286.921778	27.558682
249.648222	10297.548693	27.563700
249.662132	10315.493323	27.568717
250.153950	10317.679229	27.573735
250.168346	10345.108091	27.578752
250.593797	10356.035402	27.583770
250.967677	10372.606685	27.588788
251.514227	10393.111759	27.593805
251.536978	10408.359406	27.598823
252.038585	10431.491174	27.603840
252.027671	10438.823727	27.608858
252.305769	10442.279345	27.613876
252.525681	10458.205004	27.618893
252.835680	10467.299496	27.623911
253.227742	10482.679193	27.628928
253.115400	10504.285035	27.633946
253.104699	10513.690918	27.638964
253.449890	10536.692709	27.643981
254.241805	10534.994340	27.648999
253.844480	10578.801818	27.654016
254.223677	10574.873787	27.659034
254.945698	10604.827483	27.664052
254.903145	10618.738289	27.669069
255.291847	10631.551423	27.674087
255.390944	10653.444720	27.679104
255.677227	10679.477460	27.684122
255.993329	10683.646066	27.689140
256.090311	10714.493349	27.694157
256.704465	10723.295896	27.699175
256.443488	10739.994508	27.704192
256.631229	10746.546805	27.709210
257.200258	10770.706970	27.714228
257.131543	10791.840429	27.719245
257.342728	10812.057203	27.724263
257.974819	10826.426272	27.729280
258.341072	10835.258023	27.734298
258.508591	10859.199492	27.739316
258.601271	10888.262762	27.744333
259.203748	10897.206769	27.749351
258.981789	10919.136143	27.754368
259.065082	10943.261021	27.759386
259.819118	10956.838055	27.764404
260.025076	10985.937930	27.769421
259.922888	10996.466020	27.774439
260.502564	11011.218891	27.779456
261.260703	11025.935989	27.784474
261.448463	11044.604241	27.789492
261.731919	11058.968888	27.794509
262.197862	11067.836291	27.799527
262.256436	11082.786400	27.804544
262.500212	11093.236911	27.809562
262.766272	11106.494509	27.814580
263.002224	11111.554045	27.819597
263.331469	11116.589504	27.824615
263.101764	11144.499640	27.829632
263.049883	11143.956848	27.834650
263.712946	11160.777372	27.839668
263.456405	11175.689825	27.844685
263.691264	11195.980373	27.849703
264.057570	11226.469035	27.854720
264.415971	11246.260268	27.859738
264.826435	11263.344001	27.864756
264.958899	11289.626875	27.869773
265.555626	11309.393779	27.874791
265.409353	11321.556130	27.879808
265.577746	11343.865110	27.884826
266.314850	11349.126311	27.889844
266.317533	11379.453974	27.894861
266.737729	11407.350937	27.899879
266.545525	11423.308619	27.904896
266.863631	11438.525780	27.909914
267.381473	11469.072584	27.914932
267.270926	11497.368567	27.919949
267.944933	11504.341869	27.924967
268.116603	11540.852845	27.929984
268.209838	11570.204014	27.935002
268.477193	11591.894328	27.940020
268.786495	11615.826106	27.945037
268.932764	11634.612190	27.950055
269.582643	11675.596345	27.955072
269.816535	11688.424088	27.960090
270.051487	11712.101229	27.965108
270.200326	11730.189011	27.970125
271.004147	11749.700872	27.975143
271.213226	11774.575111	27.980160
271.665213	11782.430529	27.985178
272.201571	11818.164194	27.990196
272.079909	11828.483338	27.995213
272.637689	11826.330363	28.000231
273.066419	11841.962134	28.005248
273.052444	11866.068230	28.010266
273.232280	11877.281385	28.015284
273.337096	11900.429628	28.020301
273.859843	11902.174991	28.025319
274.297194	11926.309814	28.030336
274.168117	11938.918053	28.035354
274.708629	11954.634669	28.040372
274.596129	11987.641370	28.045389
274.930326	11992.875605	28.050407
275.230692	12013.915029	28.055424
275.128721	12044.702412	28.060442
276.019225	12044.708198	28.065460
275.749693	12071.130458	28.070477
276.539941	12090.167561	28.075495
276.766085	12099.896063	28.080512
277.210880	12133.206473	28.085530
277.867729	12139.566027	28.090548
277.844362	12161.932247	28.095565
278.574335	12173.131136	28.100583
278.333035	12182.485496	28.105600
278.656552	12184.429251	28.110618
279.094370	12210.110130	28.115636
279.125932	12219.203566	28.120653
279.889845	12232.809207	28.125671
279.920821	12254.768726	28.130688
279.480726	12271.938124	28.135706
280.134184	12284.407892	28.140724
280.087184	12311.596575	28.145741
280.343926	12316.816927	28.150759
280.678271	12338.294709	28.155776
280.810396	12362.238751	28.160794
281.302932	12368.109515	28.165812
281.262262	12398.005074	28.170829
281.559799	12423.030358	28.175847
281.894392	12425.609670	28.180864
282.315515	12455.039849	28.185882
282.584690	12473.210216	28.190900
282.520720	12497.364120	28.195917
282.613361	12524.434762	28.200935
283.116199	12541.059466	28.205952
283.597912	12568.769443	28.210970
283.800032	12592.713292	28.215988
284.119690	12628.789456	28.221005
284.425751	12648.893599	28.226023
284.918195	12666.579801	28.231040
284.808361	12693.301285	28.236058
285.382369	12699.369067	28.241076
285.590733	12732.862380	28.246093
285.903098	12757.632834	28.251111
286.127825	12773.362245	28.256128
285.917468	12807.049371	28.261146
286.744745	12824.201413	28.266164
287.137257	12852.759377	28.271181
287.099368	12871.893260	28.276199
287.487672	12908.584266	28.281216
287.571735	12939.714487	28.286234
288.098459	12955.627388	28.291252
288.464928	12989.630857	28.296269
288.882167	13003.091160	28.301287
289.369105	13023.709512	28.306304
289.835047	13047.712871	28.311322
290.322275	13061.188448	28.316340
290.491418	13076.014990	28.321357
290.881764	13095.570016	28.326375
290.758371	13097.631053	28.331392
291.259922	13125.985549	28.336410
291.937988	13138.777307	28.341428
291.971552	13157.778392	28.346445
292.149691	13174.310063	28.351463
292.756963	13189.592198	28.356480
293.251279	13198.092101	28.361498
293.708763	13207.775174	28.366516
293.959762	13218.693085	28.371533
294.017812	13224.075771	28.376551
294.719751	13242.080962	28.381568
294.390105	13260.513452	28.386586
294.558888	13276.210051	28.391604
294.670743	13294.946242	28.396621
294.781025	13309.198119	28.401639
295.271350	13322.794736	28.406656
295.391063	13358.216959	28.411674
295.874205	13380.782457	28.416692
295.880239	13403.962570	28.421709
295.604754	13420.032102	28.426727
296.387870	13442.195155	28.431744
296.719997	13484.974485	28.436762
297.516025	13504.352679	28.441780
297.505076	13517.006449	28.446797
297.578757	13535.125218	28.451815
298.503046	13542.585165	28.456832
298.525861	13576.597796	28.461850
299.120306	13582.599507	28.466868
299.377186	13606.504297	28.471885
299.338687	13625.440623	28.476903
299.745602	13648.356306	28.481920
299.579169	13666.582652	28.486938
300.243101	13690.618865	28.491956
300.503258	13706.365392	28.496973
300.540519	13739.895362	28.501991
301.229121	13745.566420	28.507008
301.362254	13767.849912	28.512026
301.268044	13782.386542	28.517044
301.569282	13817.036000	28.522061
301.740583	13833.722328	28.527079
302.168121	13862.457507	28.532096
302.543250	13886.902586	28.537114
302.764655	13916.965657	28.542132
302.815445	13934.630094	28.547149
303.296391	13978.129923	28.552167
303.418855	14004.920770	28.557184
303.660052	14038.701312	28.562202
303.947389	14065.509143	28.567220
304.621856	14097.889805	28.572237
305.189258	14111.994378	28.577255
305.878839	14140.173036	28.582272
305.913601	14158.163410	28.587290
306.381198	14173.502647	28.592308
306.982965	14194.970234	28.597325
307.296975	14214.597532	28.602343
307.561920	14218.316947	28.607360
307.519633	14252.255077	28.612378
307.771868	14272.196789	28.617396
308.554839	14281.090814	28.622413
308.560948	14304.478637	28.627431
308.655635	14317.136064	28.632448
308.680906	14354.459206	28.637466
309.219556	14364.228846	28.642484
309.936267	14391.420125	28.647501
309.704552	14427.236822	28.652519
310.425759	14445.862640	28.657536
310.312551	14459.785275	28.662554
310.544872	14485.466690	28.667572
311.097716	14530.604480	28.672589
311.383199	14553.851953	28.677607
312.155537	14571.375812	28.682624
311.869600	14595.094383	28.687642
312.182033	14610.577860	28.692660
312.632230	14648.633598	28.697677
312.795894	14666.046950	28.702695
313.675548	14688.870245	28.707712
313.602205	14720.980149	28.712730
313.860471	14743.939275	28.717748
314.471166	14765.659863	28.722765
314.905164	14798.557572	28.727783
315.123104	14804.346164	28.732800
315.351401	14832.460404	28.737818
315.221681	14851.109078	28.742836
316.008656	14878.431397	28.747853
316.283088	14919.074501	28.752871
316.788255	14935.842332	28.757888
316.923102	14946.924007	28.762906
317.281208	14980.761259	28.767924
317.549303	15001.936764	28.772941
317.994249	15024.170464	28.777959
318.225965	15049.027087	28.782976
318.546344	15070.222410	28.787994
318.982302	15079.079652	28.793012
319.515290	15095.083456	28.798029
319.560636	15129.472257	28.803047
320.168053	15149.961523	28.808064
320.284914	15168.491026	28.813082
320.263118	15185.598323	28.818100
320.631325	15200.627159	28.823117
320.879778	15233.041069	28.828135
321.382089	15254.795977	28.833152
321.460023	15267.288285	28.838170
321.791198	15291.145456	28.843188
322.485969	15315.242024	28.848205
322.603106	15340.064437	28.853223
322.946313	15356.238536	28.858240
323.278809	15369.631285	28.863258
323.404495	15406.103414	28.868276
323.563470	15422.172482	28.873293
323.803372	15449.337142	28.878311
323.983735	15479.807024	28.883328
324.583220	15519.370394	28.888346
324.810663	15532.345666	28.893364
325.169503	15551.038926	28.898381
324.987459	15592.722040	28.903399
325.211935	15609.075178	28.908416
325.828680	15648.533571	28.913434
326.497975	15695.920036	28.918452
327.010884	15716.182928	28.923469
326.986394	15748.554699	28.928487
327.677884	15766.792948	28.933504
328.019371	15797.091811	28.938522
327.855781	15833.975164	28.943540
328.983826	15858.238931	28.948557
329.047176	15874.461354	28.953575
329.568439	15910.196302	28.958592
329.619585	15932.449020	28.963610
330.258776	15954.060896	28.968628
330.493605	15967.519129	28.973645
330.728496	16006.606494	28.978663
331.129344	16029.411489	28.983680
331.225776	16056.219463	28.988698
331.510397	16077.793944	28.993716
332.215754	16090.867219	28.998733
332.200198	16127.755145	29.003751
332.811161	16153.009418	29.008768
333.028641	16179.340547	29.013786
333.417623	16216.937249	29.018804
333.657742	16234.689523	29.023821
333.850875	16259.570122	29.028839
334.271217	16290.233545	29.033856
334.541743	16321.350460	29.038874
334.688467	16343.535937	29.043892
335.439416	16373.345841	29.048909
335.635552	16408.375934	29.053927
336.036478	16420.216862	29.058944
336.873567	16455.481595	29.063962
336.752617	16476.953390	29.068980
337.324415	16504.060242	29.073997
337.699946	16532.176724	29.079015
338.034978	16556.632435	29.084032
338.275591	16576.523722	29.089050
338.500704	16606.958363	29.094068
338.946167	16627.859231	29.099085
339.043405	16655.370981	29.104103
339.986816	16674.794816	29.109120
340.515143	16692.851440	29.114138
340.380316	16715.055564	29.119156
341.425876	16719.518167	29.124173
341.932254	16737.764445	29.129191
341.850726	16742.321843	29.134208
342.436789	16770.049333	29.139226
342.441777	16780.283704	29.144244
342.843950	16795.692964	29.149261
342.754451	16812.324556	29.154279
343.237556	16841.716193	29.159296
343.479686	16858.042446	29.164314
343.445696	16886.752031	29.169332
343.857071	16898.607341	29.174349
344.168151	16924.542788	29.179367
344.114541	16943.357791	29.184384
344.860197	16970.866970	29.189402
344.943080	17004.478060	29.194420
345.556139	17023.435195	29.199437
345.082534	17056.446413	29.204455
345.835588	17086.334498	29.209472
346.060561	17117.638551	29.214490
346.079431	17153.493884	29.219508
346.574473	17178.393773	29.224525
347.161946	17227.339641	29.229543
347.499141	17256.856998	29.234560
347.946405	17278.420375	29.239578
348.307374	17321.610065	29.244596
348.840832	17354.461811	29.249613
348.809551	17385.617994	29.254631
349.474021	17422.568281	29.259648
349.877840	17443.658326	29.264666
350.149430	17476.080732	29.269684
350.442047	17499.331215	29.274701
350.637677	17534.521408	29.279719
351.156232	17571.272321	29.284736
351.692285	17599.569013	29.289754
352.209703	17638.845284	29.294772
352.324165	17667.758674	29.299789
352.276075	17708.723624	29.304807
352.935983	17727.202556	29.309824
353.077593	17772.183954	29.314842
353.565398	17815.752760	29.319860
353.683839	17839.755968	29.324877
354.395549	17884.254170	29.329895
354.647675	17916.459990	29.334912
354.541635	17944.723069	29.339930
355.245099	17993.412469	29.344948
355.490020	18026.950012	29.349965
355.998175	18060.948523	29.354983
356.446448	18096.519026	29.360000
356.880629	18128.837043	29.365018
357.238836	18168.572762	29.370036
358.013724	18181.286307	29.375053
358.251896	18225.534230	29.380071
358.836965	18249.747819	29.385088
359.367948	18269.626285	29.390106
359.536965	18302.013667	29.395124
360.363448	18321.736194	29.400141
360.138513	18342.228261	29.405159
360.552923	18364.890822	29.410176
360.592347	18388.144980	29.415194
360.991186	18427.529413	29.420212
361.520042	18452.879603	29.425229
361.881196	18485.449973	29.430247
362.514250	18514.157799	29.435264
363.019870	18555.386453	29.440282
362.933814	18577.652802	29.445300
363.335023	18584.693958	29.450317
364.174070	18623.599459	29.455335
364.133809	18656.214412	29.460352
364.730945	18671.765037	29.465370
364.745777	18705.277340	29.470388
365.286666	18730.789902	29.475405
365.520341	18761.575464	29.480423
365.903568	18790.599315	29.485440
366.255336	18825.421258	29.490458
366.088134	18853.346057	29.495476
366.711268	18889.278722	29.500493
367.576211	18917.578513	29.505511
367.761019	18948.585295	29.510528
368.002444	18966.516846	29.515546
368.218557	18993.237316	29.520564
368.678072	19023.015054	29.525581
369.145583	19060.173366	29.530599
369.476276	19081.876584	29.535616
369.877545	19111.222736	29.540634
369.749683	19141.217522	29.545652
370.398056	19165.776668	29.550669
370.674010	19197.394655	29.555687
370.942699	19232.190193	29.560704
371.204543	19260.259176	29.565722
371.811260	19296.168639	29.570740
372.327342	19315.519604	29.575757
372.741209	19349.279400	29.580775
372.968348	19379.279022	29.585792
373.187126	19414.917070	29.590810
373.817477	19445.230098	29.595828
374.046172	19480.226653	29.600845
374.485310	19517.731169	29.605863
374.540192	19549.372160	29.610880
375.120941	19587.093044	29.615898
375.523789	19623.016401	29.620916
376.361068	19643.604150	29.625933
376.472086	19688.471272	29.630951
376.557517	19720.009806	29.635968
376.927863	19751.651088	29.640986
377.449667	19786.647158	29.646004
378.034844	19825.185989	29.651021
377.814263	19850.712572	29.656039
377.964881	19901.261309	29.661056
378.675962	19924.825981	29.666074
378.871183	19970.759778	29.671092
380.119228	20003.596478	29.676109
380.552801	20043.965835	29.681127
380.656103	20075.599828	29.686144
381.138619	20104.939044	29.691162
381.414950	20133.457960	29.696180
382.158067	20153.412420	29.701197
382.890611	20195.145218	29.706215
382.972279	20219.127992	29.711232
383.586171	20242.795874	29.716250
383.921413	20272.035178	29.721268
384.022987	20298.619026	29.726285
384.590519	20306.396432	29.731303
385.083263	20347.106716	29.736320
386.088569	20365.047582	29.741338
385.845390	20387.083773	29.746356
386.118925	20416.655117	29.751373
386.402273	20437.912339	29.756391
386.710905	20473.279273	29.761408
387.395353	20507.368761	29.766426
387.381997	20530.538472	29.771444
387.738345	20557.698612	29.776461
387.823513	20604.828366	29.781479
388.003939	20631.486424	29.786496
388.433638	20667.691362	29.791514
388.628841	20707.280370	29.796532
389.454591	20768.611986	29.801549
389.567661	20792.327126	29.806567
389.905277	20838.446306	29.811584
390.577775	20863.494264	29.816602
390.810775	20912.943110	29.821620
391.374977	20953.770765	29.826637
392.040897	20984.958828	29.831655
391.990879	21023.882828	29.836672
392.522067	21044.417258	29.841690
392.826439	21105.915068	29.846708
393.262767	21122.987508	29.851725
393.695053	21149.540148	29.856743
394.113241	21191.543352	29.861760
394.456738	21224.131463	29.866778
394.760666	21263.454737	29.871796
394.796310	21291.175110	29.876813
395.117295	21327.348988	29.881831
395.436104	21375.132830	29.886848
396.267518	21408.758455	29.891866
396.614584	21449.213292	29.896884
396.908346	21497.712638	29.901901
397.698645	21524.920903	29.906919
397.683967	21561.122358	29.911936
398.354041	21592.771220	29.916954
398.470960	21629.044099	29.921972
398.777417	21669.182983	29.926989
399.359592	21720.220874	29.932007
399.512101	21767.782635	29.937024
400.067209	21795.425910	29.942042
400.356006	21843.466718	29.947060
400.494616	21890.031576	29.952077
401.140091	21924.604944	29.957095
401.177662	21981.215353	29.962112
401.866624	22019.749989	29.967130
402.572803	22078.072806	29.972148
402.705792	22124.527304	29.977165
403.052786	22161.436531	29.982183
403.647033	22189.734586	29.987200
404.448791	22230.478811	29.992218
404.642999	22286.632382	29.997236
405.291303	22322.859968	30.002253
405.610914	22361.469017	30.007271
405.838298	22415.307792	30.012288
406.421839	22459.683323	30.017306
406.604337	22489.948161	30.022324
407.212567	22535.759276	30.027341
407.621831	22565.766062	30.032359
407.801394	22613.267408	30.037376
408.223509	22648.419952	30.042394
408.857809	22690.862624	30.047412
409.396624	22742.282872	30.052429
409.851273	22776.098036	30.057447
410.357880	22819.741467	30.062464
410.758115	22849.535824	30.067482
411.173853	22893.082512	30.072500
411.632386	22924.538639	30.077517
412.607832	22949.612203	30.082535
412.787002	23001.234552	30.087552
413.099182	23029.708329	30.092570
413.604139	23048.056389	30.097588
413.948488	23088.052074	30.102605
414.191456	23120.376666	30.107623
414.404107	23156.439935	30.112640
414.986246	23193.076075	30.117658
415.513279	23230.732062	30.122676
415.601801	23267.695871	30.127693
416.058294	23295.387863	30.132711
416.228306	23344.110059	30.137728
416.944027	23373.050681	30.142746
417.646805	23410.736376	30.147764
417.881151	23451.657706	30.152781
418.371804	23491.701131	30.157799
419.057437	23517.009470	30.162816
419.834977	23540.858383	30.167834
420.236116	23582.584989	30.172852
420.441815	23601.061924	30.177869
420.737916	23631.382573	30.182887
421.317612	23660.726153	30.187904
421.645452	23693.473002	30.192922
421.695056	23739.698172	30.197940
421.901213	23762.277901	30.202957
422.447513	23779.727489	30.207975
422.364484	23829.978184	30.212992
422.675214	23873.306657	30.218010
423.178239	23905.335933	30.223028
423.469034	23950.899015	30.228045
423.910430	23986.473735	30.233063
423.708791	24034.685369	30.238080
424.048741	24085.377821	30.243098
424.461305	24133.628607	30.248116
425.258897	24183.083664	30.253133
425.926401	24247.416896	30.258151
426.167478	24291.107991	30.263168
426.627330	24346.847668	30.268186
427.201808	24397.078150	30.273204
427.742379	24455.687255	30.278221
428.166502	24480.526197	30.283239
428.207004	24539.426338	30.288256
428.909610	24580.487487	30.293274
429.511495	24624.053609	30.298292
429.759547	24678.127964	30.303309
430.481575	24717.426491	30.308327
430.723608	24769.592582	30.313344
431.228700	24815.155697	30.318362
431.530584	24863.122509	30.323380
432.046859	24919.720436	30.328397
432.657758	24962.278326	30.333415
432.854495	25022.653923	30.338432
433.324356	25067.255338	30.343450
433.740405	25112.822922	30.348468
434.183888	25164.783489	30.353485
435.165790	25200.746107	30.358503
435.249370	25257.367751	30.363520
435.726520	25295.413443	30.368538
436.418308	25345.720386	30.373556
436.752265	25391.789537	30.378573
437.433287	25420.848200	30.383591
437.902940	25469.462342	30.388608
438.262571	25506.531313	30.393626
439.416172	25542.482061	30.398644
439.304980	25585.198637	30.403661
440.352959	25616.530855	30.408679
440.648635	25648.993479	30.413696
441.263643	25667.310433	30.418714
441.944715	25706.714206	30.423732
441.715876	25742.234586	30.428749
442.454415	25771.785811	30.433767
442.434100	25809.817058	30.438784
443.021559	25848.143803	30.443802
443.444226	25891.238153	30.448820
443.396192	25920.589989	30.453837
444.167861	25965.982837	30.458855
444.755411	26005.618791	30.463872
445.385523	26042.961216	30.468890
445.747911	26084.192583	30.473908
445.997020	26129.192790	30.478925
446.336644	26162.070181	30.483943
446.604719	26201.358813	30.488960
447.009827	26256.523993	30.493978
447.251436	26300.261151	30.498996
447.178360	26342.293640	30.504013
447.963902	26390.038188	30.509031
448.414926	26445.183776	30.514048
448.742776	26495.429644	30.519066
449.297155	26545.543619	30.524084
449.741689	26599.337704	30.529101
450.446576	26650.836973	30.534119
450.641182	26689.858152	30.539136
451.129774	26732.861727	30.544154
451.481789	26777.518617	30.549172
451.950675	26830.558740	30.554189
452.313149	26875.999520	30.559207
452.930552	26928.807244	30.564224
453.531972	26964.106267	30.569242
453.921601	27021.809200	30.574260
453.959924	27074.918047	30.579277
454.558744	27105.369926	30.584295
454.859188	27160.227274	30.589312
455.353832	27205.593473	30.594330
456.097688	27243.332919	30.599348
456.239155	27311.559025	30.604365
456.871544	27345.680373	30.609383
457.426969	27396.172005	30.614400
457.976531	27457.310102	30.619418
458.410127	27497.817106	30.624436
458.804473	27563.261450	30.629453
459.400624	27607.697226	30.634471
459.516253	27664.712646	30.639488
460.088489	27700.141017	30.644506
460.844460	27755.054338	30.649524
461.017836	27828.661497	30.654541
461.477920	27859.427821	30.659559
461.870995	27915.458273	30.664576
462.631383	27968.009001	30.669594
463.529009	28009.613947	30.674612
464.076974	28071.924728	30.679629
464.648702	28092.317493	30.684647
465.040870	28136.144852	30.689664
465.610896	28184.863667	30.694682
466.377119	28207.975001	30.699700
466.971179	28247.788548	30.704717
467.676230	28282.208876	30.709735
467.994255	28321.342694	30.714752
468.235727	28360.063410	30.719770
468.884190	28390.370574	30.724788
469.150452	28437.424315	30.729805
469.617583	28470.979019	30.734823
469.851901	28513.029113	30.739840
469.905798	28556.462341	30.744858
470.377207	28604.646615	30.749876
470.513441	28665.955059	30.754893
470.842726	28718.257537	30.759911
471.351594	28764.054488	30.764928
471.950676	28818.833083	30.769946
472.611390	28867.538844	30.774964
473.173717	28917.412366	30.779981
473.703265	28960.029895	30.784999
474.310476	29018.015856	30.790016
474.930930	29062.176925	30.795034
475.722259	29101.202781	30.800052
475.782800	29151.204026	30.805069
476.267626	29199.394049	30.810087
476.403086	29241.257198	30.815104
477.127362	29288.026241	30.820122
477.977475	29335.383447	30.825140
478.160621	29396.301873	30.830157
478.384734	29429.529499	30.835175
478.827639	29489.440055	30.840192
478.977799	29533.500201	30.845210
479.816587	29592.115441	30.850228
479.838996	29657.200124	30.855245
480.169531	29696.287663	30.860263
480.793416	29747.598206	30.865280
481.605898	29821.780193	30.870298
481.704877	29863.597238	30.875316
481.768096	29923.458441	30.880333
482.542726	29983.041450	30.885351
482.932697	30044.978477	30.890368
483.302064	30093.360403	30.895386
484.122606	30145.115987	30.900404
484.730259	30198.657738	30.905421
484.957606	30252.426516	30.910439
485.530262	30312.624479	30.915456
485.547904	30367.346268	30.920474
486.758895	30420.164407	30.925492
487.124771	30475.450492	30.930509
487.592534	30527.480008	30.935527
487.935082	30582.293921	30.940544
488.244184	30647.325479	30.945562
488.748573	30696.478619	30.950580
489.178071	30760.758806	30.955597
489.947218	30833.343323	30.960615
490.727698	30880.126294	30.965632
490.818884	30937.919961	30.970650
491.423740	31001.017406	30.975668
492.015543	31065.505362	30.980685
492.688790	31119.657451	30.985703
493.320149	31168.996013	30.990720
493.570495	31236.553886	30.995738
494.503935	31269.898157	31.000756
494.737504	31337.291982	31.005773
494.952638	31395.356934	31.010791
495.483682	31457.250428	31.015808
496.003422	31519.963131	31.020826
496.635616	31570.776034	31.025844
497.259639	31627.736245	31.030861
497.818491	31677.255429	31.035879
498.317370	31738.644129	31.040896
498.729815	31785.622824	31.045914
499.411585	31850.736113	31.050932
499.745286	31906.041498	31.055949
500.136435	31963.385160	31.060967
500.817159	32030.411216	31.065984
501.188371	32080.063491	31.071002
502.256482	32126.130266	31.076020
502.977448	32180.656357	31.081037
503.535308	32216.676842	31.086055
503.825644	32273.728975	31.091072
503.962036	32322.859125	31.096090
504.650918	32368.913457	31.101108
505.202042	32427.623594	31.106125
505.577586	32490.079624	31.111143
506.271063	32532.063561	31.116160
506.443815	32595.036189	31.121178
506.915636	32634.450864	31.126196
507.548503	32694.707017	31.131213
508.019538	32747.313661	31.136231
508.981603	32792.112406	31.141248
509.484780	32841.445294	31.146266
510.089892	32886.994221	31.151284
510.580527	32951.657265	31.156301
510.682014	33003.943940	31.161319
511.047977	33055.029130	31.166336
510.891694	33110.031144	31.171354
511.524929	33175.671652	31.176372
511.991735	33239.342639	31.181389
512.770282	33301.697113	31.186407
513.043165	33373.866112	31.191424
513.769259	33432.055319	31.196442
514.170431	33501.458575	31.201460
514.678857	33565.256382	31.206477
514.794988	33623.988712	31.211495
515.324460	33684.533523	31.216512
515.687583	33760.090607	31.221530
516.510689	33805.501771	31.226548
517.027385	33882.693712	31.231565
517.592712	33940.743915	31.236583
517.926460	33990.603387	31.241600
518.377951	34066.314415	31.246618
519.145404	34126.493269	31.251636
519.461854	34180.335068	31.256653
519.793049	34255.501958	31.261671
520.788862	34310.216422	31.266688
521.171236	34380.459254	31.271706
521.842366	34435.293998	31.276724
522.265904	34503.312245	31.281741
522.718279	34561.067591	31.286759
523.340052	34623.357952	31.291776
523.553662	34702.673510	31.296794
524.165581	34766.944491	31.301812
524.638948	34822.333752	31.306829
525.140134	34891.558683	31.311847
525.989801	34959.022337	31.316864
526.448941	35022.540061	31.321882
527.516712	35094.815115	31.326900
527.937771	35163.413761	31.331917
528.629197	35204.337801	31.336935
529.690839	35251.849592	31.341952
529.945042	35321.981621	31.346970
530.699639	35359.178294	31.351988
531.349639	35427.695964	31.357005
531.754836	35473.798928	31.362023
532.174514	35525.633395	31.367040
532.414895	35596.399911	31.372058
532.887103	35635.190070	31.377076
533.415123	35699.629745	31.382093
533.552255	35772.957476	31.387111
534.386840	35828.631014	31.392128
534.492621	35895.075570	31.397146
535.293032	35966.385343	31.402164
535.636726	36028.909580	31.407181
535.889520	36106.151597	31.412199
536.451387	36170.350698	31.417216
536.952368	36239.946959	31.422234
537.846896	36315.199893	31.427252
538.551011	36384.154099	31.432269
539.270280	36453.345908	31.437287
539.645146	36515.683660	31.442304
540.013377	36585.195891	31.447322
540.888675	36642.742950	31.452340
541.470339	36720.005875	31.457357
541.641666	36784.088643	31.462375
541.986278	36843.324017	31.467392
542.615042	36921.056561	31.472410
543.405381	36986.735669	31.477428
543.605666	37059.256632	31.482445
543.992698	37130.052317	31.487463
544.651063	37181.662797	31.492480
545.365100	37266.025963	31.497498
546.106106	37338.165236	31.502516
546.997851	37402.519395	31.507533
547.535658	37473.323087	31.512551
548.393839	37518.955683	31.517568
549.054315	37581.474031	31.522586
549.562033	37643.165706	31.527604
550.143263	37696.182201	31.532621
550.706436	37747.125173	31.537639
551.881706	37804.752650	31.542656
551.891964	37845.899390	31.547674
552.623425	37902.312822	31.552692
552.955015	37955.721634	31.557709
553.539461	37994.286901	31.562727
553.952135	38041.948012	31.567744
554.314793	38104.921343	31.572762
554.806109	38158.216003	31.577780
555.502834	38204.088462	31.582797
555.906224	38251.426581	31.587815
556.621036	38299.978988	31.592832
557.010455	38372.010042	31.597850
557.720999	38417.757673	31.602868
558.202203	38469.590474	31.607885
557.979845	38535.063758	31.612903
558.793933	38606.154501	31.617920
559.346603	38663.139546	31.622938
559.663263	38738.712685	31.627956
560.337720	38800.440741	31.632973
561.098113	38860.914421	31.637991
561.443795	38920.838182	31.643008
562.058056	38996.189647	31.648026
562.912553	39050.724162	31.653044
563.180315	39118.482626	31.658061
563.747569	39204.113186	31.663079
564.342164	39263.198428	31.668096
564.786227	39327.182043	31.673114
565.486550	39404.948180	31.678132
566.233711	39461.670044	31.683149
566.755044	39540.419534	31.688167
567.493889	39599.030687	31.693184
567.908959	39665.838896	31.698202
568.106050	39737.335837	31.703220
568.634429	39806.379492	31.708237
569.187203	39887.101181	31.713255
569.931848	39962.542435	31.718272
570.369260	40047.507158	31.723290
570.862082	40117.318562	31.728308
571.383442	40191.411970	31.733325
571.784897	40269.265885	31.738343
572.705110	40339.670404	31.743360
573.084750	40439.863844	31.748378
573.329027	40509.316924	31.753396
574.286705	40582.168791	31.758413
575.160539	40674.387458	31.763431
575.529469	40743.937633	31.768448
575.747696	40829.507217	31.773466
576.301007	40912.496600	31.778484
577.254470	40986.322998	31.783501
577.980470	41063.195498	31.788519
578.633188	41133.022252	31.793536
578.981614	41222.612624	31.798554
579.774222	41294.418185	31.803572
580.866687	41367.755982	31.808589
581.224903	41444.921265	31.813607
581.967271	41505.021588	31.818624
582.538586	41588.127855	31.823642
582.886657	41646.270331	31.828660
583.669360	41717.593055	31.833677
584.113308	41806.640174	31.838695
584.622585	41868.869938	31.843712
585.345074	41958.635716	31.848730
585.794545	42031.962414	31.853748
586.243378	42093.776759	31.858765
586.603576	42187.641004	31.863783
587.303232	42254.572654	31.868800
587.775618	42334.791222	31.873818
588.332957	42401.664835	31.878836
589.157619	42483.063341	31.883853
589.163183	42565.257275	31.888871
590.043731	42641.833052	31.893888
590.780534	42725.311728	31.898906
591.221988	42801.689200	31.903924
592.124722	42861.789569	31.908941
592.387208	42944.829846	31.913959
593.098579	43004.772872	31.918976
593.992956	43082.992955	31.923994
594.059149	43160.696667	31.929012
595.014637	43226.342592	31.934029
595.026271	43313.264825	31.939047
595.653336	43382.387714	31.944064
596.347630	43468.547583	31.949082
596.984350	43542.733315	31.954100
597.704287	43615.172389	31.959117
598.206796	43709.971127	31.964135
599.237041	43771.843441	31.969152
599.603691	43859.505175	31.974170
600.045002	43928.619740	31.979188
600.660667	44011.366526	31.984205
601.152988	44097.932058	31.989223
602.250427	44170.683492	31.994240
602.738323	44250.841505	31.999258
603.250822	44337.730007	32.004276
604.720350	44397.072432	32.009293
605.192045	44482.424497	32.014311
605.988859	44539.422200	32.019328
606.140004	44615.327840	32.024346
606.407616	44687.763719	32.029364
607.607554	44756.819210	32.034381
608.385169	44846.605677	32.039399
608.516506	44907.080036	32.044416
608.856601	44980.281763	32.049434
609.210979	45065.289631	32.054452
610.240949	45137.130907	32.059469
611.120032	45219.631176	32.064487
611.560708	45294.241466	32.069504
612.308869	45368.832842	32.074522
612.591939	45452.272426	32.079540
613.292939	45542.633744	32.084557
614.150519	45619.812870	32.089575
614.703004	45686.348649	32.094592
615.380130	45765.045305	32.099610
616.129974	45845.277412	32.104628
616.801316	45906.022600	32.109645
617.371668	45988.551993	32.114663
617.778158	46071.456132	32.119680
618.617882	46145.318740	32.124698
619.338817	46222.323999	32.129716
620.055977	46296.570555	32.134733
620.626921	46375.022081	32.139751
621.278117	46431.910682	32.144768
622.144257	46511.390733	32.149786
622.722837	46583.725753	32.154804
623.347612	46655.532428	32.159821
623.800169	46727.721466	32.164839
623.746840	46803.458187	32.169856
624.789702	46876.718603	32.174874
625.274241	46965.117459	32.179892
625.872166	47034.568132	32.184909
625.948493	47128.163129	32.189927
626.653492	47205.838149	32.194944
627.600961	47294.503117	32.199962
627.756481	47380.305832	32.204980
627.975141	47478.959744	32.209997
628.816194	47576.181987	32.215015
629.542497	47655.371034	32.220032
630.223995	47753.315236	32.225050
630.796492	47849.800124	32.230068
632.043643	47924.593957	32.235085
632.374662	48016.114531	32.240103
633.173877	48087.774694	32.245120
633.574500	48161.389321	32.250138
634.179072	48241.147224	32.255156
634.547315	48331.336893	32.260173
635.217474	48411.122573	32.265191
635.825752	48500.161842	32.270208
636.386307	48585.003131	32.275226
636.546234	48671.669905	32.280244
637.581448	48767.855677	32.285261
638.080430	48862.927334	32.290279
638.236562	48955.987648	32.295296
639.111850	49056.969768	32.300314
639.691853	49158.301199	32.305332
640.699317	49237.662003	32.310349
641.318819	49333.739291	32.315367
642.347720	49438.898196	32.320384
643.253927	49517.878982	32.325402
644.011399	49600.371132	32.330420
644.634637	49680.883604	32.335437
645.082757	49774.461821	32.340455
646.011960	49860.883789	32.345472
646.783992	49945.986758	32.350490
646.838894	50034.132952	32.355508
648.135974	50116.389780	32.360525
648.346410	50222.275587	32.365543
649.159590	50318.363740	32.370560
649.613551	50392.069765	32.375578
649.643480	50495.166649	32.380596
650.484905	50582.247485	32.385613
651.060393	50680.404272	32.390631
651.669254	50777.144322	32.395648
652.671841	50874.738883	32.400666
653.364358	50988.005915	32.405684
654.109353	51069.309475	32.410701
654.795386	51165.356548	32.415719
655.460986	51253.309573	32.420736
656.195507	51355.621987	32.425754
656.753748	51448.890148	32.430772
657.314966	51552.378706	32.435789
657.866914	51653.746925	32.440807
658.451948	51740.047859	32.445824
659.422456	51848.855464	32.450842
659.649637	51956.453592	32.455860
660.699507	52038.197290	32.460877
661.504149	52140.120116	32.465895
662.444921	52239.582661	32.470912
663.105928	52317.418412	32.475930
663.495825	52410.453710	32.480948
664.444748	52504.628950	32.485965
665.513994	52593.724818	32.490983
666.291233	52672.850434	32.496000
667.183652	52753.568212	32.501018
668.063627	52830.573910	32.506036
668.739523	52917.746337	32.511053
669.386096	52985.953498	32.516071
669.747205	53071.403476	32.521088
670.189299	53156.783600	32.526106
670.723510	53242.995399	32.531124
671.619000	53318.459060	32.536141
672.119071	53409.339396	32.541159
672.445043	53493.445126	32.546176
673.190838	53572.238468	32.551194
673.647589	53675.130207	32.556212
674.389072	53758.385102	32.561229
674.952773	53858.215144	32.566247
675.674814	53956.048488	32.571264
676.657547	54036.415540	32.576282
677.317739	54147.760608	32.581300
678.016500	54221.004893	32.586317
678.421628	54294.228454	32.591335
679.023918	54376.441302	32.596352
679.774909	54469.344688	32.601370
680.343783	54555.765055	32.606388
680.982924	54651.000051	32.611405
681.752053	54736.611065	32.616423
682.066602	54827.812947	32.621440
683.111291	54911.553381	32.626458
683.642206	55018.363304	32.631476
683.881542	55106.331534	32.636493
684.402434	55194.708548	32.641511
685.235142	55290.167401	32.646528
686.060144	55390.903485	32.651546
686.524174	55493.557189	32.656564
687.277907	55595.013705	32.661581
687.902502	55706.089201	32.666599
688.924060	55798.840482	32.671616
689.397887	55898.032367	32.676634
689.867040	56012.635504	32.681652
690.601644	56122.286232	32.686669
691.611231	56218.472246	32.691687
692.245213	56333.125844	32.696704
693.032845	56423.934769	32.701722
693.661456	56523.199012	32.706740
694.272607	56645.560229	32.711757
694.892269	56742.539806	32.716775
695.650950	56856.739880	32.721792
696.727642	56959.704418	32.726810
697.194551	57060.931515	32.731828
698.023389	57165.884154	32.736845
699.089640	57272.365144	32.741863
699.551900	57378.567339	32.746880
700.066645	57481.627395	32.751898
700.618919	57583.392782	32.756916
701.170788	57683.692821	32.761933
701.980298	57798.749271	32.766951
702.535410	57919.604796	32.771968
703.590153	58016.348145	32.776986
704.167157	58135.267812	32.782004
704.427365	58242.430540	32.787021
705.375799	58357.113420	32.792039
705.821194	58482.015619	32.797056
706.910160	58573.378604	32.802074
707.670823	58688.833722	32.807092
708.711854	58808.009358	32.812109
709.721559	58913.326812	32.817127
710.181540	59026.078418	32.822144
711.255638	59124.643857	32.827162
711.855763	59228.596167	32.832180
712.608911	59331.936059	32.837197
713.380653	59427.766152	32.842215
714.381238	59525.972873	32.847232
714.773538	59622.150927	32.852250
715.568183	59730.699448	32.857268
716.419699	59825.627243	32.862285
717.636777	59916.286398	32.867303
718.025359	60016.031092	32.872320
719.011938	60106.678617	32.877338
719.645597	60205.991974	32.882356
719.955031	60299.791871	32.887373
720.908622	60388.234283	32.892391
721.379886	60491.633016	32.897408
722.305708	60596.859414	32.902426
722.729731	60704.261033	32.907444
723.443301	60793.503220	32.912461
724.589195	60895.370686	32.917479
724.679981	60989.608041	32.922496
725.522830	61083.974426	32.927514
726.126910	61179.461368	32.932532
726.811376	61277.431815	32.937549
728.004768	61363.424732	32.942567
728.527738	61455.140781	32.947584
729.420313	61551.390781	32.952602
730.074703	61644.665962	32.957620
730.663699	61735.329587	32.962637
731.631316	61836.573962	32.967655
731.497219	61939.068867	32.972672
732.496960	62033.609692	32.977690
733.198425	62148.310743	32.982708
733.779732	62239.432936	32.987725
734.581473	62355.161415	32.992743
734.936325	62461.079571	32.997760
735.400934	62577.035631	33.002778
736.072216	62694.247554	33.007796
736.803081	62818.402642	33.012813
737.966774	62927.090666	33.017831
738.636922	63044.917865	33.022848
739.711800	63157.180152	33.027866
740.401476	63261.928462	33.032884
740.920125	63375.636380	33.037901
741.757196	63484.981758	33.042919
742.603194	63614.924902	33.047936
742.893877	63734.013320	33.052954
743.614051	63848.954703	33.057972
744.366338	63965.857151	33.062989
744.800753	64104.227273	33.068007
745.303573	64234.894691	33.073024
745.916360	64370.651968	33.078042
746.762018	64497.623670	33.083060
747.792434	64636.499429	33.088077
748.416450	64766.151510	33.093095
749.168776	64918.273139	33.098112
750.209880	65024.963510	33.103130
751.202466	65163.210647	33.108148
751.472451	65299.435199	33.113165
752.492721	65416.573438	33.118183
752.845586	65567.381494	33.123200
753.757295	65710.146303	33.128218
754.778701	65839.202194	33.133236
755.354148	65963.041633	33.138253
756.524775	66103.250531	33.143271
756.936220	66228.269115	33.148288
757.528555	66374.909338	33.153306
758.632434	66498.702637	33.158324
759.381722	66641.734573	33.163341
760.508189	66763.521813	33.168359
761.050645	66888.687092	33.173376
761.862486	67026.344346	33.178394
762.482631	67159.394088	33.183412
763.333289	67280.218435	33.188429
764.346161	67410.613042	33.193447
765.019397	67544.933459	33.198464
765.958077	67665.372516	33.203482
766.756968	67799.465198	33.208500
767.782966	67927.148798	33.213517
768.595886	68042.723996	33.218535
769.534816	68168.583775	33.223552
770.392852	68287.263263	33.228570
771.459765	68390.476918	33.233588
772.273960	68513.122498	33.238605
773.124910	68622.536946	33.243623
773.774752	68743.345999	33.248640
774.386567	68854.653522	33.253658
775.075134	68963.413767	33.258676
775.691999	69072.205382	33.263693
776.408669	69173.799014	33.268711
776.978795	69297.184914	33.273728
777.601268	69421.681939	33.278746
778.496254	69532.668099	33.283764
778.993065	69650.681534	33.288781
779.332926	69762.512934	33.293799
780.147563	69885.356098	33.298816
780.807632	70011.544804	33.303834
781.486840	70141.423457	33.308852
781.971060	70271.802974	33.313869
782.633504	70392.164150	33.318887
783.615396	70542.783997	33.323904
784.793701	70668.815164	33.328922
786.022865	70808.799252	33.333940
786.536055	70943.212004	33.338957
787.594144	71063.334610	33.343975
788.139385	71186.843102	33.348992
788.643852	71331.761980	33.354010
789.705119	71457.665397	33.359028
790.347374	71594.090595	33.364045
791.345522	71716.876101	33.369063
792.001193	71852.851803	33.374080
793.019995	71994.908111	33.379098
793.832071	72125.434520	33.384116
794.505471	72265.488324	33.389133
795.555562	72395.572393	33.394151
795.960385	72545.226721	33.399168
796.829676	72673.205075	33.404186
797.703973	72806.583473	33.409204
798.523548	72940.047617	33.414221
799.046184	73088.579685	33.419239
799.724897	73234.722037	33.424256
800.289668	73371.493824	33.429274
801.618133	73519.680797	33.434292
802.142974	73659.603796	33.439309
803.070236	73802.028632	33.444327
804.120713	73946.040267	33.449344
804.681698	74100.593077	33.454362
805.603381	74237.235521	33.459380
806.255839	74378.982303	33.464397
807.113661	74521.707910	33.469415
807.864327	74663.522544	33.474432
808.817671	74812.792132	33.479450
809.717920	74967.048457	33.484468
810.354666	75101.226460	33.489485
811.479895	75243.741904	33.494503
812.857948	75387.133521	33.499520
813.209144	75540.890113	33.504538
814.357296	75674.506564	33.509556
815.119838	75800.788209	33.514573
815.753676	75937.324432	33.519591
816.947803	76082.072750	33.524608
817.836668	76220.484881	33.529626
818.740883	76347.505205	33.534644
819.496454	76495.440251	33.539661
820.430719	76619.731378	33.544679
821.241240	76747.079384	33.549696
822.248706	76884.185929	33.554714
823.322757	77006.470270	33.559732
824.230649	77143.835210	33.564749
825.036623	77261.118224	33.569767
825.810974	77383.213813	33.574784
826.656189	77502.749531	33.579802
827.363160	77622.624960	33.584820
827.915238	77760.210612	33.589837
828.913330	77891.879367	33.594855
829.660794	78011.636374	33.599872
830.436023	78143.337102	33.604890
831.427979	78260.929933	33.609908
831.713448	78381.340793	33.614925
832.138997	78517.554235	33.619943
833.134323	78639.835321	33.624960
833.334360	78773.026267	33.629978
834.486486	78915.921593	33.634996
835.078380	79044.185472	33.640013
836.136721	79188.812144	33.645031
836.841368	79320.613735	33.650048
837.413182	79463.772858	33.655066
838.509225	79605.790015	33.660084
838.981618	79759.366205	33.665101
840.097012	79898.364850	33.670119
840.998818	80035.653819	33.675136
841.897227	80187.555953	33.680154
842.455928	80346.447940	33.685172
843.183008	80490.144636	33.690189
843.755695	80637.631457	33.695207
845.184538	80802.765491	33.700224
846.108619	80936.324184	33.705242
846.881632	81090.429157	33.710260
847.576881	81250.336076	33.715277
848.265834	81398.150273	33.720295
848.810441	81550.550191	33.725312
849.410601	81713.664309	33.730330
850.920279	81861.706595	33.735348
851.618503	82029.317171	33.740365
852.679617	82178.257973	33.745383
853.991197	82329.340881	33.750400
855.244955	82501.854469	33.755418
856.162195	82633.532827	33.760436
856.898597	82781.645552	33.765453
858.055212	82927.235287	33.770471
858.906425	83072.509461	33.775488
859.396206	83219.887632	33.780506
860.516159	83372.249070	33.785524
861.245329	83523.739749	33.790541
862.242771	83667.557483	33.795559
863.204341	83807.472298	33.800576
863.737841	83958.359196	33.805594
864.694726	84102.743095	33.810612
865.608301	84257.055123	33.815629
866.491944	84409.203102	33.820647
867.272637	84562.261148	33.825664
867.754579	84721.082555	33.830682
868.987357	84870.341577	33.835700
869.747261	85030.555394	33.840717
870.517024	85183.049965	33.845735
871.569018	85350.265864	33.850752
872.411854	85479.340903	33.855770
873.376284	85639.069639	33.860788
874.412353	85796.781991	33.865805
875.008170	85943.565393	33.870823
875.871405	86098.189109	33.875840
876.641553	86265.299987	33.880858
877.711044	86409.679747	33.885876
878.335337	86574.817553	33.890893
878.965421	86729.901571	33.895911
880.198494	86880.540208	33.900928
880.987317	87050.089653	33.905946
882.035496	87194.186745	33.910964
882.834244	87355.688351	33.915981
883.726816	87519.396522	33.920999
884.442919	87674.839614	33.926016
885.155020	87842.844589	33.931034
886.280097	88008.903283	33.936052
886.978440	88162.739009	33.941069
887.830900	88329.711876	33.946087
888.732920	88473.543581	33.951104
889.498991	88633.312939	33.956122
890.528431	88781.206897	33.961140
891.222737	88939.269019	33.966157
891.898313	89087.799164	33.971175
892.735585	89249.212522	33.976192
893.638106	89415.577342	33.981210
894.780504	89570.323452	33.986228
895.385928	89741.643835	33.991245
895.794801	89905.923087	33.996263
897.165994	90077.005549	34.001280
897.722335	90243.832021	34.006298
898.593998	90401.368370	34.011316
899.437767	90585.704323	34.016333
900.357110	90754.543790	34.021351
901.853876	90916.359542	34.026368
902.550287	91109.476024	34.031386
903.253030	91267.191543	34.036404
904.142132	91447.096742	34.041421
905.093211	91632.992539	34.046439
906.235933	91807.827365	34.051456
907.477860	91963.034585	34.056474
909.356617	92118.257908	34.061492
910.232566	92274.217398	34.066509
911.014881	92444.907766	34.071527
912.145013	92596.156737	34.076544
912.633727	92761.404413	34.081562
913.668399	92913.645783	34.086580
914.608777	93084.023451	34.091597
915.409745	93237.311752	34.096615
916.600384	93399.074545	34.101632
917.486013	93560.236886	34.106650
918.626652	93702.858204	34.111668
919.406169	93881.306013	34.116685
920.221549	94042.464170	34.121703
920.942790	94196.980581	34.126720
921.733982	94367.942550	34.131738
922.515299	94537.356664	34.136756
923.455474	94703.321538	34.141773
924.351260	94887.884358	34.146791
925.507565	95061.449258	34.151808
926.299746	95224.378650	34.156826
927.277724	95393.715597	34.161844
928.269340	95561.000675	34.166861
928.872301	95733.478069	34.171879
930.391863	95911.299496	34.176896
931.446071	96081.438803	34.181914
932.070573	96247.757427	34.186932
933.175725	96412.807811	34.191949
933.886187	96580.310821	34.196967
934.873865	96753.472432	34.201984
935.313097	96940.582054	34.207002
936.012891	97110.635056	34.212020
937.020839	97292.317257	34.217037
937.643802	97471.190497	34.222055
938.881194	97670.397230	34.227072
939.466217	97848.956618	34.232090
940.232159	98026.183390	34.237108
941.282143	98241.403119	34.242125
941.782656	98429.273463	34.247143
943.687877	98610.722191	34.252160
944.274903	98807.127091	34.257178
944.942750	98986.605183	34.262196
946.051988	99188.516652	34.267213
947.203882	99382.503168	34.272231
948.192626	99570.149524	34.277248
948.814697	99766.252274	34.282266
949.654494	99954.825044	34.287284
951.088195	100122.017179	34.292301
951.668257	100303.285439	34.297319
952.677460	100482.673525	34.302336
953.509808	100671.423809	34.307354
954.865905	100862.190895	34.312372
955.650264	101035.941176	34.317389
956.420726	101215.038323	34.322407
957.354761	101399.630417	34.327424
958.039180	101593.312225	34.332442
958.828089	101770.783141	34.337460
960.334282	101973.183121	34.342477
960.542250	102166.080566	34.347495
961.798361	102354.950647	34.352512
962.678985	102554.843688	34.357530
964.146280	102749.519322	34.362548
965.310046	102951.483396	34.367565
966.058833	103137.600181	34.372583
967.313986	103320.456276	34.377600
968.272055	103525.282685	34.382618
969.578107	103708.519357	34.387636
970.637537	103887.467178	34.392653
971.458549	104088.584992	34.397671
972.863643	104267.763303	34.402688
973.670124	104453.303855	34.407706
974.421092	104647.333268	34.412724
975.607667	104836.119036	34.417741
976.217167	105035.987403	34.422759
977.377451	105214.826417	34.427776
977.954282	105427.873756	34.432794
978.632095	105614.722904	34.437812
979.994603	105819.392989	34.442829
980.865549	106031.237900	34.447847
981.519952	106228.556094	34.452864
982.617856	106437.251344	34.457882
983.453510	106648.296526	34.462900
984.537336	106853.159996	34.467917
985.169729	107063.482173	34.472935
986.503350	107276.324573	34.477952
987.888467	107477.330979	34.482970
989.061167	107676.081583	34.487988
990.748043	107881.436061	34.493005
991.253356	108098.183414	34.498023
992.836786	108275.909478	34.503040
993.686597	108469.209845	34.508058
995.133628	108654.155003	34.513076
995.992652	108835.601450	34.518093
996.946991	109038.198009	34.523111
998.227994	109210.128615	34.528128
999.453806	109389.175068	34.533146
1000.587923	109578.586056	34.538164
1002.066414	109752.704107	34.543181
1002.620451	109933.157050	34.548199
1003.915419	110105.901734	34.553216
1004.824499	110281.535850	34.558234
1005.716306	110460.087259	34.563252
1006.798032	110623.788580	34.568269
1007.779440	110811.232131	34.573287
1008.388084	110987.275103	34.578304
1009.455186	111167.550255	34.583322
1010.230026	111363.493183	34.588340
1011.399502	111542.297225	34.593357
1011.874592	111740.547086	34.598375
1012.554896	111935.192359	34.603392
1013.576975	112124.449666	34.608410
1014.604622	112322.207176	34.613428
1015.734657	112513.412799	34.618445
1016.362231	112714.659412	34.623463
1017.373415	112893.029735	34.628480
1018.242983	113098.660220	34.633498
1019.167162	113298.570036	34.638516
1020.249592	113477.806471	34.643533
1021.220501	113689.163202	34.648551
1022.283033	113873.460031	34.653568
1023.079412	114066.403723	34.658586
1023.996347	114270.438934	34.663604
1025.257398	114463.574713	34.668621
1026.058970	114659.346722	34.673639
1027.507949	114863.007079	34.678656
1028.196543	115061.017563	34.683674
1029.347867	115264.577975	34.688692
1030.452787	115464.891647	34.693709
1031.248016	115674.493519	34.698727
1032.099659	115879.096059	34.703744
1032.933004	116106.216110	34.708762
1033.585196	116324.765512	34.713780
1034.487273	116537.460147	34.718797
1035.387333	116770.149040	34.723815
1036.514262	116998.887519	34.728832
1037.650754	117235.937539	34.733850
1038.525723	117458.133131	34.738868
1039.880599	117672.662018	34.743885
1040.448751	117926.168370	34.748903
1041.516333	118162.971446	34.753920
1042.565358	118393.001032	34.758938
1043.861510	118628.604590	34.763956
1045.139496	118859.575745	34.768973
1045.683023	119098.196260	34.773991
1046.839923	119332.042065	34.779008
1048.267736	119578.122911	34.784026
1049.387822	119823.407725	34.789044
1050.587993	120054.566059	34.794061
1051.072213	120298.591435	34.799079
1052.471805	120541.998920	34.804096
1053.385599	120784.234204	34.809114
1054.282373	121026.347606	34.814132
1056.038604	121245.398593	34.819149
1057.461361	121500.163849	34.824167
1058.853737	121731.569915	34.829184
1059.880530	121954.560804	34.834202
1060.895034	122193.053023	34.839220
1061.939083	122406.211190	34.844237
1063.265601	122637.483225	34.849255
1064.745429	122869.922945	34.854272
1065.737645	123082.055458	34.859290
1067.058535	123314.284150	34.864308
1067.831811	123526.341947	34.869325
1068.600881	123764.038352	34.874343
1069.953085	123987.383755	34.879360
1070.828423	124209.821094	34.884378
1071.437484	124433.102438	34.889396
1072.352783	124669.641393	34.894413
1073.476909	124925.474010	34.899431
1074.236751	125150.801519	34.904448
1075.307404	125396.191714	34.909466
1076.089434	125643.050968	34.914484
1077.266748	125881.102367	34.919501
1078.127114	126131.273113	34.924519
1079.529631	126392.889388	34.929536
1080.559422	126628.347602	34.934554
1081.808823	126878.257524	34.939572
1083.062321	127115.076704	34.944589
1084.073445	127356.145503	34.949607
1084.979865	127602.898809	34.954624
1086.278120	127845.622403	34.959642
1087.257220	128083.964612	34.964660
1088.857634	128323.891800	34.969677
1089.709803	128563.804968	34.974695
1090.802920	128765.631160	34.979712
1092.038901	128997.410650	34.984730
1093.327574	129223.048602	34.989748
1094.625374	129440.333973	34.994765
1095.655839	129651.264163	34.999783
1096.763111	129892.070808	35.004800
1098.224176	130101.057067	35.009818
1098.938328	130321.664439	35.014836
1100.116249	130533.324110	35.019853
1101.351092	130769.680133	35.024871
1101.878175	131000.286034	35.029888
1102.897208	131227.656202	35.034906
1103.531655	131473.230381	35.039924
1104.785670	131710.845223	35.044941
1105.577805	131956.790090	35.049959
1106.257913	132208.814477	35.054976
1107.247421	132463.553176	35.059994
1108.155585	132730.539854	35.065012
1109.399124	132986.901398	35.070029
1110.512802	133253.972631	35.075047
1111.353014	133522.168746	35.080064
1112.667213	133774.823425	35.085082
1113.559093	134051.128460	35.090100
1115.011817	134309.139403	35.095117
1116.025142	134585.847322	35.100135
1116.947683	134859.961137	35.105152
1118.175958	135124.480937	35.110170
1119.226018	135402.723719	35.115188
1120.633016	135678.970332	35.120205
1121.770183	135948.164470	35.125223
1122.924273	136234.358627	35.130240
1124.312274	136502.197464	35.135258
1125.458470	136769.076866	35.140276
1126.785934	137041.253218	35.145293
1127.883406	137305.482672	35.150311
1128.958301	137587.556014	35.155328
1130.198310	137853.084844	35.160346
1130.935229	138141.583148	35.165364
1132.472781	138416.411271	35.170381
1133.513964	138687.000239	35.175399
1135.183152	138953.493979	35.180416
1136.701433	139206.448558	35.185434
1137.957215	139471.708769	35.190452
1139.297596	139739.188598	35.195469
1140.336962	139999.683406	35.200487
1141.251790	140259.249854	35.205504
1143.068037	140511.569155	35.210522
1143.939521	140777.422932	35.215540
1145.050817	141017.385963	35.220557
1146.074993	141287.795784	35.225575
1147.062754	141556.146993	35.230592
1148.612809	141808.202878	35.235610
1149.475654	142078.772392	35.240628
1150.535985	142346.242915	35.245645
1151.636441	142600.864098	35.250663
1152.601892	142863.497881	35.255680
1153.769770	143127.114659	35.260698
1154.405996	143409.169526	35.265716
1155.823356	143670.580934	35.270733
1156.689564	143953.071428	35.275751
1158.027247	144229.894260	35.280768
1159.258870	144490.302675	35.285786
1160.683488	144773.151446	35.290804
1162.031119	145031.667984	35.295821
1163.297140	145296.299424	35.300839
1164.807542	145550.329214	35.305856
1166.349377	145794.819444	35.310874
1167.672873	146053.689847	35.315892
1168.497294	146286.711273	35.320909
1169.535433	146530.376666	35.325927
1170.301715	146770.081258	35.330944
1171.419786	147011.986703	35.335962
1172.316862	147280.308071	35.340980
1173.274672	147532.021030	35.345997
1173.897369	147795.141299	35.351015
1174.491787	148063.531150	35.356032
1176.309363	148339.774168	35.361050
1176.611915	148622.382157	35.366068
1177.501292	148913.265737	35.371085
1178.748642	149191.790706	35.376103
1179.601683	149500.972872	35.381120
1180.778301	149799.565059	35.386138
1181.685459	150114.387188	35.391156
1182.980863	150409.946259	35.396173
1184.294823	150731.377627	35.401191
1185.363518	151030.606378	35.406208
1186.665222	151326.552220	35.411226
1188.005288	151650.726779	35.416244
1189.461297	151957.382112	35.421261
1191.318101	152253.751011	35.426279
1192.176468	152558.848396	35.431296
1193.675117	152857.906657	35.436314
1194.462662	153164.961223	35.441332
1196.299415	153466.835002	35.446349
1197.886642	153762.664115	35.451367
1198.944732	154053.712229	35.456384
1200.521227	154354.925712	35.461402
1201.636991	154656.927931	35.466420
1202.895451	154954.938797	35.471437
1204.170195	155244.438077	35.476455
1204.762491	155554.182407	35.481472
1206.046012	155846.475328	35.486490
1207.284585	156160.544732	35.491508
1208.309577	156480.169795	35.496525
1209.325228	156773.959954	35.501543
1210.649035	157096.445559	35.506560
1211.934872	157400.013968	35.511578
1213.488597	157711.456035	35.516596
1214.556710	158031.606687	35.521613
1215.860747	158322.354380	35.526631
1217.186838	158635.211295	35.531648
1218.466380	158930.420064	35.536666
1219.504004	159249.114010	35.541684
1220.581636	159568.653828	35.546701
1222.138144	159873.617215	35.551719
1223.090781	160190.670796	35.556736
1224.792350	160493.661281	35.561754
1226.076923	160806.097908	35.566772
1227.089960	161113.456512	35.571789
1228.692008	161430.184203	35.576807
1229.734353	161736.870272	35.581824
1231.396212	162036.123563	35.586842
1232.575001	162349.794629	35.591860
1233.551403	162646.222185	35.596877
1234.868502	162954.330905	35.601895
1236.001504	163278.216722	35.606912
1237.203856	163562.434084	35.611930
1238.475013	163876.418569	35.616948
1239.937599	164187.341568	35.621965
1241.440926	164469.980238	35.626983
1242.987916	164773.090956	35.632000
1244.302131	165066.346063	35.637018
1245.579161	165356.830761	35.642036
1246.861766	165659.534678	35.647053
1248.087867	165939.006206	35.652071
1249.474032	166208.442481	35.657088
1250.932793	166483.438424	35.662106
1252.013834	166750.479691	35.667124
1253.240604	167047.366125	35.672141
1254.692158	167315.263247	35.677159
1255.406162	167581.114075	35.682176
1256.308067	167873.009858	35.687194
1257.464290	168153.674492	35.692212
1258.819750	168444.306503	35.697229
1259.749176	168725.875027	35.702247
1260.618603	169026.208967	35.707264
1261.710246	169324.592269	35.712282
1262.679693	169630.001931	35.717300
1263.618482	169957.890683	35.722317
1265.295503	170269.697295	35.727335
1266.084037	170584.342787	35.732352
1267.552262	170903.522499	35.737370
1268.515120	171239.030052	35.742388
1269.594834	171556.311645	35.747405
1271.043922	171888.152646	35.752423
1271.835468	172240.839193	35.757440
1273.388702	172553.532067	35.762458
1274.489921	172902.898650	35.767476
1275.601888	173255.641566	35.772493
1277.444613	173587.125236	35.777511
1278.592806	173932.469102	35.782528
1280.312425	174275.919205	35.787546
1281.318809	174609.794273	35.792564
1282.839094	174954.411631	35.797581
1284.354591	175288.067850	35.802599
1285.851803	175626.107609	35.807616
1287.390560	175954.104720	35.812634
1288.725835	176296.186120	35.817652
1289.599522	176645.338687	35.822669
1291.297275	176964.788294	35.827687
1292.332349	177313.830192	35.832704
1293.806389	177650.466545	35.837722
1294.949326	177990.814868	35.842740
1296.085085	178330.240276	35.847757
1297.497681	178686.742740	35.852775
1298.617982	179037.889517	35.857792
1300.111219	179371.183907	35.862810
1301.725596	179727.064005	35.867828
1302.491932	180075.458966	35.872845
1303.832277	180413.024466	35.877863
1305.301657	180784.965474	35.882880
1306.574676	181124.399796	35.887898
1308.247210	181466.626105	35.892916
1309.789292	181812.836118	35.897933
1311.216561	182154.561719	35.902951
1312.003061	182499.060677	35.907968
1312.915582	182862.807919	35.912986
1314.528689	183199.788188	35.918004
1315.737122	183553.464447	35.923021
1317.580930	183903.890472	35.928039
1318.739148	184262.034812	35.933056
1320.392672	184599.410786	35.938074
1321.616907	184943.091868	35.943092
1322.728538	185287.479141	35.948109
1324.105348	185637.866658	35.953127
1325.519098	185994.761835	35.958144
1326.974014	186344.569825	35.963162
1328.219577	186699.276072	35.968180
1329.136526	187048.136489	35.973197
1330.777717	187391.167588	35.978215
1331.898027	187752.628703	35.983232
1332.852687	188106.211468	35.988250
1334.035050	188458.248346	35.993268
1335.144751	188817.179352	35.998285
1336.673852	189157.523305	36.003303
1337.692995	189509.162056	36.008320
1338.810606	189867.654088	36.013338
1340.191229	190215.695920	36.018356
1341.010048	190585.717038	36.023373
1342.423531	190940.079410	36.028391
1344.285938	191295.029936	36.033408
1345.481901	191655.360709	36.038426
1347.360213	192027.475642	36.043444
1348.447578	192403.544462	36.048461
1350.131005	192763.573007	36.053479
1351.314547	193135.530234	36.058496
1352.614495	193491.640333	36.063514
1353.992054	193866.451712	36.068532
1355.008349	194243.280013	36.073549
1356.687817	194600.628815	36.078567
1357.746046	194976.223281	36.083584
1359.154505	195342.126702	36.088602
1360.603023	195728.680567	36.093620
1362.140052	196098.858134	36.098637
1363.666813	196467.414575	36.103655
1365.042894	196855.777325	36.108672
1366.236868	197220.660624	36.113690
1367.793164	197599.654334	36.118708
1368.889477	197988.806438	36.123725
1370.787079	198346.737073	36.128743
1372.331641	198737.800183	36.133760
1373.677081	199119.617878	36.138778
1375.111673	199483.229937	36.143796
1376.089006	199864.515959	36.148813
1377.670094	200252.115974	36.153831
1379.273362	200635.004322	36.158848
1380.729703	201027.288811	36.163866
1382.084877	201396.459792	36.168884
1383.361102	201774.787087	36.173901
1385.081210	202152.027487	36.178919
1386.068401	202532.730037	36.183936
1387.810411	202913.145029	36.188954
1389.298879	203302.973954	36.193972
1390.679435	203675.276125	36.198989
1392.280145	204056.647409	36.204007
1393.532850	204442.737847	36.209024
1394.664074	204817.854959	36.214042
1396.130991	205203.342723	36.219060
1397.400329	205596.737215	36.224077
1399.083300	205971.007337	36.229095
1400.172101	206370.428702	36.234112
1401.362604	206765.353318	36.239130
1402.872429	207154.221523	36.244148
1403.956191	207550.551833	36.249165
1405.883534	207924.232612	36.254183
1407.195170	208335.639170	36.259200
1408.228110	208737.050205	36.264218
1409.710195	209125.844018	36.269236
1411.574565	209519.300154	36.274253
1413.176196	209900.180135	36.279271
1414.884123	210289.577236	36.284288
1416.287261	210678.582089	36.289306
1418.281320	211057.726651	36.294324
1419.464791	211440.600234	36.299341
1421.346752	211820.592164	36.304359
1422.155424	212199.112208	36.309376
1423.310976	212572.141942	36.314394
1424.398202	212965.222210	36.319412
1425.855090	213373.404896	36.324429
1427.429167	213756.961006	36.329447
1428.669528	214151.215043	36.334464
1429.350232	214536.369612	36.339482
1430.859447	214907.624070	36.344500
1431.781151	215312.297761	36.349517
1433.331342	215690.405868	36.354535
1434.653114	216083.867708	36.359552
1435.624140	216495.903704	36.364570
1437.332976	216891.641672	36.369588
1438.179489	217307.714600	36.374605
1439.812569	217712.967191	36.379623
1441.525711	218125.268851	36.384640
1442.730021	218539.586487	36.389658
1444.518959	218948.094893	36.394676
1445.956704	219365.577657	36.399693
1447.316125	219779.138407	36.404711
1448.581174	220200.742278	36.409728
1450.074467	220657.436121	36.414746
1452.004442	221110.275580	36.419764
1453.062307	221524.172593	36.424781
1454.665803	221952.102851	36.429799
1456.182161	222380.836588	36.434816
1457.562623	222813.709090	36.439834
1459.067518	223235.184069	36.444852
1460.535710	223675.589023	36.449869
1461.956712	224099.062294	36.454887
1463.544927	224535.869580	36.459904
1464.525869	224989.796327	36.464922
1466.430637	225417.690396	36.469940
1467.368515	225863.626876	36.474957
1469.086454	226307.480555	36.479975
1470.659232	226764.212110	36.484992
1471.542529	227221.694173	36.490010
1473.150819	227661.456172	36.495028
1475.208377	228105.895399	36.500045
1477.517990	228544.554189	36.505063
1479.636371	228989.062695	36.510080
1480.955082	229420.775961	36.515098
1482.697360	229838.196564	36.520116
1484.142934	230263.109772	36.525133
1486.372653	230689.190354	36.530151
1487.743861	231110.384625	36.535168
1489.061004	231541.139753	36.540186
1490.650868	231955.569329	36.545204
1492.351977	232372.369433	36.550221
1493.689383	232786.335059	36.555239
1495.009799	233205.765866	36.560256
1496.447020	233642.095670	36.565274
1498.160397	234060.498789	36.570292
1499.398274	234494.933452	36.575309
1500.660848	234920.373211	36.580327
1501.958283	235339.407230	36.585344
1503.702143	235776.073432	36.590362
1505.142396	236206.770756	36.595380
1506.489965	236645.358956	36.600397
1508.198052	237071.391224	36.605415
1509.630755	237507.529033	36.610432
1510.655120	237950.365147	36.615450
1512.509386	238378.306987	36.620468
1513.689505	238831.077042	36.625485
1514.961495	239276.669704	36.630503
1516.861361	239729.958197	36.635520
1518.171600	240174.733764	36.640538
1519.757886	240609.507169	36.645556
1520.528299	241071.494782	36.650573
1522.001318	241517.465727	36.655591
1523.589441	241978.583737	36.660608
1524.485907	242452.086151	36.665626
1525.798940	242909.695180	36.670644
1527.011954	243386.348005	36.675661
1529.052659	243840.028436	36.680679
1530.750318	244297.805316	36.685696
1531.918899	244757.702544	36.690714
1533.620235	245205.116238	36.695732
1535.105251	245664.734235	36.700749
1536.192905	246131.404307	36.705767
1537.758307	246599.469679	36.710784
1539.085491	247074.891103	36.715802
1540.691164	247541.096929	36.720820
1541.711086	248022.972030	36.725837
1543.512478	248512.797009	36.730855
1544.854439	248995.407888	36.735872
1546.595177	249479.757241	36.740890
1548.372471	249960.011332	36.745908
1550.394379	250444.188533	36.750925
1552.407840	250924.989118	36.755943
1554.147460	251379.797329	36.760960
1555.825077	251855.548368	36.765978
1557.406081	252344.220610	36.770996
1558.868223	252816.908992	36.776013
1561.053857	253295.676792	36.781031
1562.566633	253781.745128	36.786048
1563.944085	254261.790238	36.791066
1565.595595	254737.649769	36.796084
1566.527254	255226.533244	36.801101
1567.992768	255703.211611	36.806119
1569.726482	256209.923445	36.811136
1570.970085	256693.065999	36.816154
1572.571136	257203.661544	36.821172
1573.829524	257712.815061	36.826189
1574.894450	258216.310352	36.831207
1576.959964	258714.941090	36.836224
1578.528617	259230.445516	36.841242
1580.118230	259745.692548	36.846260
1581.500071	260272.075171	36.851277
1583.103059	260786.989846	36.856295
1585.405581	261287.588644	36.861312
1587.127124	261817.344650	36.866330
1588.571629	262326.899862	36.871348
1590.391959	262839.949423	36.876365
1591.820974	263350.827924	36.881383
1593.389700	263859.523927	36.886400
1594.768009	264381.943510	36.891418
1596.762027	264883.913251	36.896436
1598.309847	265412.705970	36.901453
1599.667172	265930.733429	36.906471
1601.404346	266438.587395	36.911488
1603.270432	266957.571729	36.916506
1604.772919	267491.501901	36.921524
1606.271772	267998.225434	36.926541
1608.030631	268522.789406	36.931559
1609.847220	269053.059023	36.936576
1611.400426	269562.820444	36.941594
1613.065812	270091.259429	36.946612
1614.600857	270612.885871	36.951629
1616.070749	271125.148707	36.956647
1618.030572	271649.574256	36.961664
1619.864307	272171.123942	36.966682
1621.503114	272680.486250	36.971700
1622.897433	273206.704809	36.976717
1624.095501	273732.396040	36.981735
1625.827778	274251.698371	36.986752
1627.235243	274796.633913	36.991770
1628.474244	275313.602514	36.996788
1630.319375	275854.932853	37.001805
1632.058659	276393.358279	37.006823
1633.465475	276917.078600	37.011840
1635.195736	277447.171285	37.016858
1636.433113	277978.284030	37.021876
1638.226899	278494.849857	37.026893
1639.945105	279015.186530	37.031911
1641.664133	279523.811436	37.036928
1642.801570	280054.707185	37.041946
1644.534267	280572.726140	37.046964
1646.285945	281084.796587	37.051981
1647.772064	281615.961006	37.056999
1649.592130	282139.067292	37.062016
1651.622366	282675.549624	37.067034
1653.241960	283202.115279	37.072052
1654.924749	283734.562167	37.077069
1656.537029	284261.760963	37.082087
1658.474308	284777.956487	37.087104
1660.234645	285313.002095	37.092122
1661.889576	285841.941646	37.097140
1663.621481	286382.576759	37.102157
1665.044999	286914.751522	37.107175
1666.781006	287452.943774	37.112192
1668.480837	287980.928897	37.117210
1669.801689	288524.316836	37.122228
1671.658909	289070.814773	37.127245
1673.040542	289621.580222	37.132263
1675.377915	290164.286250	37.137280
1676.946719	290707.421764	37.142298
1678.071762	291262.160114	37.147316
1679.760034	291817.743051	37.152333
1681.586452	292377.110875	37.157351
1683.228684	292930.029641	37.162368
1685.009998	293500.245831	37.167386
1686.530760	294058.488268	37.172404
1688.439912	294622.937820	37.177421
1690.076651	295202.847237	37.182439
1691.630453	295760.136553	37.187456
1693.004541	296336.197589	37.192474
1694.602391	296907.138969	37.197492
1696.497312	297489.508846	37.202509
1697.920109	298089.275660	37.207527
1699.773299	298655.721106	37.212544
1701.171331	299251.853547	37.217562
1702.981163	299842.911182	37.222580
1704.890310	300422.392811	37.227597
1706.529310	301023.910640	37.232615
1708.707851	301603.214131	37.237632
1709.758840	302198.751800	37.242650
1711.593034	302793.318528	37.247668
1713.674095	303393.707743	37.252685
1715.495179	303996.015497	37.257703
1716.953219	304597.388807	37.262720
1718.648514	305197.550820	37.267738
1720.296219	305790.453223	37.272756
1722.057926	306390.799606	37.277773
1723.415263	307008.757758	37.282791
1725.276423	307624.952296	37.287808
1727.058972	308231.123907	37.292826
1728.423691	308844.877426	37.297844
1730.333194	309460.212761	37.302861
1731.884363	310081.088173	37.307879
1733.418635	310683.448360	37.312896
1734.837136	311315.307218	37.317914
1737.344612	311935.604448	37.322932
1739.975752	312536.652463	37.327949
1741.851494	313147.851448	37.332967
1743.701531	313750.949010	37.337984
1745.175408	314359.944610	37.343002
1746.967213	314956.135019	37.348020
1748.772039	315572.735303	37.353037
1750.136460	316177.188742	37.358055
1751.731202	316761.411355	37.363072
1753.125174	317354.677042	37.368090
1754.942605	317953.327511	37.373108
1756.710101	318527.680172	37.378125
1758.273424	319131.263461	37.383143
1759.955008	319716.514046	37.388160
1762.066464	320314.156371	37.393178
1764.103650	320919.423347	37.398196
1766.175196	321521.327533	37.403213
1767.684235	322118.545501	37.408231
1769.428668	322699.697320	37.413248
1771.112088	323300.532211	37.418266
1772.320012	323912.535833	37.423284
1774.306740	324522.069239	37.428301
1775.868244	325135.526330	37.433319
1777.670752	325748.099850	37.438336
1779.168079	326385.777579	37.443354
1780.815007	327023.043244	37.448372
1782.682239	327649.043863	37.453389
1783.913836	328286.644187	37.458407
1785.648803	328925.221075	37.463424
1787.596380	329572.388191	37.468442
1789.234220	330223.077534	37.473460
1791.331232	330880.234027	37.478477
1792.791400	331548.074831	37.483495
1795.041740	332190.466281	37.488512
1796.868856	332836.372971	37.493530
1798.601801	333509.096334	37.498548
1800.773500	334150.209162	37.503565
1802.399614	334826.437615	37.508583
1804.274079	335481.648017	37.513600
1806.435147	336140.788817	37.518618
1807.890680	336803.160368	37.523636
1809.929541	337470.276047	37.528653
1811.442925	338150.213145	37.533671
1813.487721	338818.224702	37.538688
1815.206825	339484.504562	37.543706
1816.930363	340163.619270	37.548724
1818.902613	340842.455519	37.553741
1820.432527	341513.816931	37.558759
1822.710073	342195.046861	37.563776
1824.289798	342882.626686	37.568794
1826.633897	343547.480940	37.573812
1828.680020	344203.618703	37.578829
1830.375782	344885.795896	37.583847
1832.363869	345539.107902	37.588864
1834.692468	346229.968893	37.593882
1836.478343	346898.853996	37.598900
1838.570811	347570.064777	37.603917
1840.064132	348239.106022	37.608935
1841.768039	348908.661265	37.613952
1843.957565	349571.680502	37.618970
1845.597913	350246.277163	37.623988
1847.750835	350902.710131	37.629005
1849.441490	351581.136110	37.634023
1851.562400	352248.543261	37.639040
1853.573373	352910.807040	37.644058
1855.600515	353581.813126	37.649076
1857.426443	354226.171848	37.654093
1859.247583	354893.918272	37.659111
1861.241784	355566.980045	37.664128
1863.061538	356217.552475	37.669146
1864.574667	356889.404077	37.674164
1866.680758	357552.063272	37.679181
1868.852016	358208.484715	37.684199
1870.246295	358874.539024	37.689216
1871.974552	359548.469293	37.694234
1873.661230	360205.852519	37.699252
1875.291130	360858.058648	37.704269
1877.001965	361512.067739	37.709287
1878.477957	362164.227513	37.714304
1880.433765	362819.697254	37.719322
1882.557695	363476.752209	37.724340
1884.662182	364133.469672	37.729357
1886.040707	364801.864486	37.734375
1887.715508	365466.571225	37.739392
1889.241794	366140.195537	37.744410
1890.640053	366824.483915	37.749428
1892.205508	367504.699033	37.754445
1893.896612	368209.792075	37.759463
1896.034054	368918.375110	37.764480
1897.883823	369620.726752	37.769498
1899.548833	370333.647917	37.774516
1901.617537	371039.538681	37.779533
1903.393260	371764.285081	37.784551
1905.157485	372488.942965	37.789568
1906.922822	373217.365485	37.794586
1908.738629	373950.533350	37.799604
1910.530020	374687.088928	37.804621
1912.356912	375434.047409	37.809639
1914.294033	376184.826992	37.814656
1916.715648	376936.220792	37.819674
1918.393271	377678.819566	37.824692
1920.687966	378424.039620	37.829709
1923.012143	379180.295569	37.834727
1924.456669	379929.199030	37.839744
1926.549502	380695.730118	37.844762
1928.150488	381454.590835	37.849780
1930.342612	382219.676318	37.854797
1932.345979	382989.643967	37.859815
1933.922308	383750.155659	37.864832
1936.215861	384516.997257	37.869850
1937.839533	385314.813887	37.874868
1939.850456	386081.031622	37.879885
1941.843654	386864.956513	37.884903
1943.729618	387646.598251	37.889920
1945.916057	388432.430603	37.894938
1947.906595	389214.244921	37.899956
1949.759514	389999.611817	37.904973
1951.698412	390784.944931	37.909991
1953.709548	391563.706098	37.915008
1955.999710	392350.538895	37.920026
1957.735987	393149.458320	37.925044
1959.642421	393932.841212	37.930061
1961.524048	394743.608676	37.935079
1963.307728	395534.524122	37.940096
1965.720624	396338.849862	37.945114
1967.582392	397138.201187	37.950132
1969.857434	397940.833759	37.955149
1972.198355	398725.971674	37.960167
1974.224976	399526.599953	37.965184
1976.631069	400308.618261	37.970202
1978.419920	401106.175986	37.975220
1980.587474	401869.261135	37.980237
1982.841465	402666.775057	37.985255
1984.693761	403442.946128	37.990272
1986.485364	404219.004695	37.995290
1988.549607	405001.509030	38.000308
1990.708396	405783.798664	38.005325
1992.586826	406576.754274	38.010343
1994.944155	407380.883012	38.015360
1996.896548	408150.446692	38.020378
1998.545576	408937.976057	38.025396
2000.561469	409721.064802	38.030413
2002.619188	410507.848174	38.035431
2004.273616	411288.291378	38.040448
2005.946831	412047.252678	38.045466
2008.120480	412817.838375	38.050484
2009.970732	413585.846117	38.055501
2012.101444	414348.035522	38.060519
2013.919367	415124.666795	38.065536
2015.814756	415889.104741	38.070554
2017.681027	416677.358436	38.075572
2019.377216	417443.151402	38.080589
2021.394617	418218.923210	38.085607
2022.970545	419029.490804	38.090624
2025.063711	419826.955998	38.095642
2027.463413	420620.091317	38.100660
2029.107881	421411.249923	38.105677
2031.561802	422224.432418	38.110695
2033.483572	423028.231511	38.115712
2036.013711	423824.105711	38.120730
2038.312513	424643.160084	38.125748
2040.383771	425426.651915	38.130765
2042.456770	426237.360728	38.135783
2044.130619	427049.425040	38.140800
2046.592737	427850.800709	38.145818
2048.776821	428677.511247	38.150836
2050.357042	429478.522783	38.155853
2052.524621	430297.636668	38.160871
2054.506171	431127.283330	38.165888
2056.826518	431934.013747	38.170906
2058.781632	432768.366057	38.175924
2060.898571	433596.587673	38.180941
2063.221353	434419.684211	38.185959
2064.616987	435251.408253	38.190976
2066.859986	436080.634466	38.195994
2068.705821	436928.471477	38.201012
2070.497034	437776.235625	38.206029
2072.952924	438632.766013	38.211047
2074.563707	439501.245711	38.216064
2076.513630	440345.294899	38.221082
2078.530239	441221.080615	38.226100
2080.798039	442074.121157	38.231117
2083.095027	442921.052317	38.236135
2085.243098	443800.358373	38.241152
2087.228426	444670.447871	38.246170
2089.199580	445536.457804	38.251188
2091.509509	446419.528243	38.256205
2093.677546	447292.569538	38.261223
2095.921252	448177.704260	38.266240
2097.686124	449052.461022	38.271258
2100.112613	449929.652825	38.276276
2102.164677	450800.092471	38.281293
2104.403344	451682.200167	38.286311
2106.292459	452572.926910	38.291328
2108.475697	453457.447931	38.296346
2110.402559	454346.677236	38.301364
2112.564488	455225.867464	38.306381
2114.902892	456110.604534	38.311399
2116.730512	457022.693913	38.316416
2119.914887	457897.253301	38.321434
2122.015241	458778.931710	38.326452
2124.173403	459643.220432	38.331469
2126.821140	460518.362696	38.336487
2128.408993	461413.409106	38.341504
2130.699141	462274.833606	38.346522
2132.905614	463152.714573	38.351540
2134.454071	464052.957508	38.356557
2136.792618	464920.022414	38.361575
2138.624857	465804.722268	38.366592
2140.907092	466703.005088	38.371610
2142.800927	467582.813230	38.376628
2144.739994	468476.168858	38.381645
2146.596406	469352.567758	38.386663
2148.622422	470224.603700	38.391680
2150.775632	471084.451839	38.396698
2152.492984	471972.629213	38.401716
2154.508973	472850.156119	38.406733
2156.708729	473742.617772	38.411751
2158.146282	474634.657853	38.416768
2160.776150	475523.377483	38.421786
2162.546643	476431.746634	38.426804
2164.086521	477344.352867	38.431821
2166.623805	478258.770360	38.436839
2168.386868	479185.493583	38.441856
2170.443562	480110.253125	38.446874
2172.166365	481062.747795	38.451892
2174.193674	482022.919848	38.456909
2176.512600	482953.249581	38.461927
2178.445358	483919.295871	38.466944
2181.082976	484880.377396	38.471962
2183.465420	485838.925085	38.476980
2185.609575	486812.102169	38.481997
2187.922046	487791.761388	38.487015
2189.986759	488766.106732	38.492032
2192.528541	489735.826992	38.497050
2194.507251	490719.013384	38.502068
2196.586733	491718.380472	38.507085
2198.900127	492689.539450	38.512103
2200.856161	493681.142536	38.517120
2203.240588	494677.159928	38.522138
2205.884403	495668.737129	38.527156
2208.088402	496668.150611	38.532173
2210.946135	497658.466966	38.537191
2212.931995	498666.326141	38.542208
2215.503439	499653.142264	38.547226
2217.876448	500633.677776	38.552244
2219.928659	501635.395447	38.557261
2222.665855	502614.291889	38.562279
2224.750524	503621.382851	38.567296
2227.024962	504606.240157	38.572314
2229.475998	505587.781814	38.577332
2231.577535	506590.855664	38.582349
2233.894135	507571.392857	38.587367
2235.766543	508581.945936	38.592384
2237.561917	509582.868927	38.597402
2240.176333	510598.719815	38.602420
2242.074883	511603.231057	38.607437
2244.671667	512614.974444	38.612455
2246.855087	513626.570531	38.617472
2249.000019	514640.578277	38.622490
2251.320438	515653.635218	38.627508
2253.790132	516672.146058	38.632525
2256.721581	517672.523849	38.637543
2259.008637	518680.552809	38.642560
2261.462277	519673.725347	38.647578
2263.897261	520684.320667	38.652596
2266.145998	521696.996481	38.657613
2268.965233	522679.133626	38.662631
2271.060974	523692.508892	38.667648
2272.935245	524688.424849	38.672666
2275.306974	525676.235312	38.677684
2276.981284	526699.150010	38.682701
2279.384396	527698.104600	38.687719
2281.887705	528703.875172	38.692736
2283.804967	529719.795911	38.697754
2286.434131	530732.408175	38.702772
2288.404601	531738.212615	38.707789
2291.057423	532756.069668	38.712807
2293.207916	533772.227534	38.717824
2295.439421	534771.035948	38.722842
2297.806193	535753.948930	38.727860
2299.453407	536752.768176	38.732877
2301.520742	537732.224450	38.737895
2303.415055	538729.557941	38.742912
2305.592596	539729.694132	38.747930
2307.881931	540746.598056	38.752948
2309.848166	541745.973959	38.757965
2312.086315	542757.711489	38.762983
2314.209051	543791.781774	38.768000
2316.156209	544815.543665	38.773018
2318.673728	545853.421659	38.778036
2320.967825	546902.676406	38.783053
2323.357038	547937.352863	38.788071
2325.158137	548996.388102	38.793088
2327.706432	550056.878493	38.798106
2330.297284	551099.582075	38.803124
2332.504896	552167.910106	38.808141
2335.383568	553229.961287	38.813159
2337.378983	554299.163065	38.818176
2339.821186	555363.482267	38.823194
2342.537773	556439.282450	38.828212
2344.145301	557518.395973	38.833229
2347.009113	558605.657896	38.838247
2349.618157	559687.647730	38.843264
2351.799741	560773.488910	38.848282
2354.242429	561869.748427	38.853300
2355.840323	562971.833358	38.858317
2358.790843	564070.438577	38.863335
2360.806052	565182.014200	38.868352
2363.007145	566288.492690	38.873370
2365.489601	567393.022949	38.878388
2367.581739	568528.906949	38.883405
2369.881942	569654.112927	38.888423
2372.108958	570787.968236	38.893440
2374.309381	571932.721517	38.898458
2376.937572	573071.479003	38.903476
2378.891707	574217.021512	38.908493
2381.610861	575374.027851	38.913511
2383.881328	576545.705434	38.918528
2386.321638	577689.698571	38.923546
2388.629429	578849.012112	38.928564
2391.342565	580013.870293	38.933581
2393.602077	581174.279750	38.938599
2396.368167	582334.697606	38.943616
2398.804073	583499.373975	38.948634
2401.763329	584671.877539	38.953652
2404.215277	585829.910900	38.958669
2406.869427	586977.823213	38.963687
2409.082393	588132.969357	38.968704
2411.842533	589293.730150	38.973722
2414.628750	590440.339876	38.978740
2416.589259	591608.528049	38.983757
2419.515850	592767.722886	38.988775
2422.167907	593909.461922	38.993792
2424.070680	595060.885193	38.998810
2426.504791	596206.196995	39.003828
2428.862082	597378.261704	39.008845
2431.532936	598525.863710	39.013863
2434.117364	599683.685220	39.018880
2436.134647	600852.402995	39.023898
2438.818733	602017.788639	39.028916
2440.750736	603188.388378	39.033933
2443.088732	604345.935523	39.038951
2445.842669	605519.116786	39.043968
2448.169943	606681.085820	39.048986
2450.953187	607840.659180	39.054004
2453.410466	609016.382782	39.059021
2455.776099	610171.332883	39.064039
2458.598020	611309.027628	39.069056
2460.602262	612444.590842	39.074074
2463.135285	613573.098464	39.079092
2465.188964	614702.571554	39.084109
2467.602171	615833.771417	39.089127
2469.792647	616977.395189	39.094144
2471.662197	618137.055136	39.099162
2474.131166	619281.994462	39.104180
2476.405419	620451.493664	39.109197
2478.804359	621620.397474	39.114215
2481.464197	622798.130025	39.119232
2483.478237	623978.640193	39.124250
2486.111990	625156.370967	39.129268
2488.209843	626359.244921	39.134285
2490.608091	627570.578150	39.139303
2493.251551	628778.087298	39.144320
2495.181536	629999.613459	39.149338
2497.852289	631213.735300	39.154356
2500.067560	632454.560186	39.159373
2502.721788	633686.279025	39.164391
2505.365652	634917.106567	39.169408
2507.713561	636173.198212	39.174426
2510.696187	637417.404170	39.179444
2512.945944	638678.002253	39.184461
2515.557601	639922.668236	39.189479
2517.948743	641197.857251	39.194496
2520.422474	642470.829331	39.199514
2522.769035	643735.134339	39.204532
2525.415568	645022.925662	39.209549
2527.987342	646301.240600	39.214567
2529.987607	647604.620931	39.219584
2532.532864	648885.356934	39.224602
2535.486517	650180.120731	39.229620
2538.248056	651476.294521	39.234637
2540.835260	652791.168519	39.239655
2543.619274	654085.255698	39.244672
2546.351760	655392.038051	39.249690
2548.882118	656692.354110	39.254708
2551.070188	657998.532790	39.259725
2553.776116	659303.854873	39.264743
2556.855759	660622.686171	39.269760
2558.934810	661941.603744	39.274778
2561.682096	663247.935038	39.279796
2564.087070	664566.940018	39.284813
2566.636516	665893.754420	39.289831
2569.229603	667220.677226	39.294848
2571.783427	668545.581729	39.299866
2574.500874	669866.643569	39.304884
2576.861092	671200.564421	39.309901
2579.603076	672529.061952	39.314919
2582.344010	673866.871536	39.319936
2584.619282	675209.142413	39.324954
2587.357219	676546.173315	39.329972
2589.842320	677901.596431	39.334989
2592.353848	679230.525317	39.340007
2595.048472	680573.645469	39.345024
2597.533169	681937.573604	39.350042
2600.128364	683284.638633	39.355060
2602.728834	684638.558863	39.360077
2605.331783	685995.953684	39.365095
2607.778842	687355.009537	39.370112
2609.954552	688714.552340	39.375130
2612.875439	690076.151124	39.380148
2615.339097	691455.240670	39.385165
2618.208048	692832.662300	39.390183
2620.704106	694195.444298	39.395200
2623.041668	695560.723543	39.400218
2626.161888	696914.354163	39.405236
2628.243520	698266.858126	39.410253
2630.508998	699612.033312	39.415271
2633.829951	700938.681603	39.420288
2636.167426	702275.504008	39.425306
2639.200600	703613.494472	39.430324
2641.652992	704959.651859	39.435341
2644.566375	706281.491567	39.440359
2647.501360	707609.963144	39.445376
2649.875555	708966.212255	39.450394
2652.113778	710306.024179	39.455412
2655.189876	711651.480751	39.460429
2657.345652	713007.869218	39.465447
2659.755739	714369.445382	39.470464
2662.035582	715749.039856	39.475482
2664.853632	717120.748603	39.480500
2667.416660	718506.675360	39.485517
2669.931815	719914.941305	39.490535
2672.443035	721303.630042	39.495552
2674.910377	722713.954851	39.500570
2677.948635	724115.589498	39.505588
2680.137672	725529.388132	39.510605
2682.278398	726968.113352	39.515623
2685.324852	728387.657017	39.520640
2687.896709	729826.502380	39.525658
2690.975483	731279.239628	39.530676
2693.501294	732728.351025	39.535693
2696.286550	734172.073911	39.540711
2699.315035	735625.424115	39.545728
2702.009692	737091.600876	39.550746
2704.927635	738548.143883	39.555764
2707.494658	740019.531941	39.560781
2710.244788	741479.861567	39.565799
2713.055713	742946.030182	39.570816
2715.557817	744442.411465	39.575834
2718.582028	745908.883146	39.580852
2721.090674	747393.606734	39.585869
2723.865039	748868.540271	39.590887
2726.655865	750345.903308	39.595904
2729.357023	751837.685457	39.600922
2731.750860	753334.305922	39.605940
2734.631518	754836.221085	39.610957
2737.513708	756338.040058	39.615975
2740.249070	757820.779816	39.620992
2743.033523	759323.703664	39.626010
2745.865267	760832.180530	39.631028
2748.780500	762355.156309	39.636045
2751.472314	763858.379067	39.641063
2754.032169	765365.406783	39.646080
2756.488911	766896.149488	39.651098
2759.237135	768423.286071	39.656116
2762.149159	769945.511268	39.661133
2764.752293	771483.302238	39.666151
2767.342332	773018.958139	39.671168
2770.123538	774567.331802	39.676186
2773.031699	776097.970511	39.681204
2775.386886	777645.618270	39.686221
2778.105485	779188.361386	39.691239
2781.208507	780736.605005	39.696256
2784.045203	782293.347193	39.701274
2786.840350	783842.695510	39.706292
2789.587171	785393.779163	39.711309
2791.653824	786970.536288	39.716327
2794.681393	788521.828894	39.721344
2797.883724	790087.560750	39.726362
2800.558806	791651.172104	39.731380
2803.526311	793231.982176	39.736397
2806.359818	794788.944272	39.741415
2809.578748	796330.852945	39.746432
2812.281479	797875.592714	39.751450
2814.925467	799384.896638	39.756468
2817.708752	800895.808506	39.761485
2820.313469	802425.360101	39.766503
2823.242073	803943.658278	39.771520
2825.790366	805473.327008	39.776538
2828.435669	806990.412860	39.781556
2831.314439	808528.197999	39.786573
2833.956594	810066.017954	39.791591
2836.666407	811605.531901	39.796608
2839.923686	813166.691622	39.801626
2842.205474	814714.071133	39.806644
2844.669387	816280.210159	39.811661
2847.547283	817859.294426	39.816679
2850.355956	819436.992343	39.821696
2853.084954	821018.576147	39.826714
2856.596771	822589.847287	39.831732
2859.956769	824169.746435	39.836749
2862.626337	825751.917267	39.841767
2865.729667	827342.656369	39.846784
2868.294802	828952.352827	39.851802
2871.212375	830548.631634	39.856820
2874.014372	832146.487160	39.861837
2876.527636	833758.415041	39.866855
2879.587072	835381.343933	39.871872
2881.831266	837015.488328	39.876890
2884.531073	838648.558048	39.881908
2887.274390	840291.033509	39.886925
2889.430539	841947.242157	39.891943
2892.579956	843606.795311	39.896960
2895.313047	845289.466885	39.901978
2898.201590	846972.636744	39.906996
2900.913058	848656.454764	39.912013
2903.510523	850348.681591	39.917031
2906.567318	852049.117087	39.922048
2909.626864	853756.079943	39.927066
2912.451298	855457.369437	39.932084
2915.704929	857167.243739	39.937101
2918.669880	858897.844058	39.942119
2922.060980	860599.270227	39.947136
2925.187469	862314.522584	39.952154
2928.061415	864014.888549	39.957172
2931.271595	865745.641702	39.962189
2933.874241	867467.279762	39.967207
2936.999672	869183.690917	39.972224
2940.014094	870907.861808	39.977242
2942.520829	872640.430126	39.982260
2945.645054	874364.748189	39.987277
2948.534338	876108.730387	39.992295
2951.140089	877827.000756	39.997312
2954.133949	879588.318569	40.002330
2956.660630	881342.419711	40.007348
2959.487390	883088.312521	40.012365
2962.295002	884860.738377	40.017383
2964.976891	886632.935569	40.022400
2967.761628	888406.119763	40.027418
2970.718405	890179.504373	40.032436
2974.207034	891960.650725	40.037453
2977.482321	893747.550023	40.042471
2980.425801	895521.988576	40.047488
2983.614921	897302.197263	40.052506
2986.161728	899091.013224	40.057524
2989.479922	900865.167682	40.062541
2992.081384	902661.804636	40.067559
2995.278813	904433.218033	40.072576
2998.260455	906223.453377	40.077594
3001.559796	908020.567639	40.082612
3004.548931	909789.642950	40.087629
3007.019323	911546.123611	40.092647
3009.967630	913298.602952	40.097664
3013.469742	915036.211198	40.102682
3016.134919	916777.922414	40.107700
3019.024904	918520.290618	40.112717
3022.374875	920253.385826	40.117735
3025.486955	922006.218025	40.122752
3028.143842	923752.513499	40.127770
3030.950537	925513.277487	40.132788
3034.395205	927263.484355	40.137805
3037.065435	929042.289571	40.142823
3040.087154	930802.910199	40.147840
3043.056908	932591.980048	40.152858
3045.964845	934372.700932	40.157876
3049.060963	936154.035539	40.162893
3051.658739	937955.710022	40.167911
3054.868832	939757.526485	40.172928
3057.454133	941570.204510	40.177946
3060.212758	943380.312279	40.182964
3063.530821	945215.115029	40.187981
3066.223737	947063.221218	40.192999
3069.662466	948893.450817	40.198016
3072.823800	950730.615510	40.203034
3075.468296	952587.721603	40.208052
3078.941988	954450.024968	40.213069
3081.757446	956367.213334	40.218087
3084.736072	958285.568545	40.223104
3087.753246	960222.442978	40.228122
3090.640269	962158.492786	40.233140
3093.760049	964108.411776	40.238157
3096.503357	966063.006527	40.243175
3098.974436	968013.662112	40.248192
3102.127288	969993.605750	40.253210
3104.974036	971977.990649	40.258228
3108.019958	973962.729093	40.263245
3110.848376	975978.407169	40.268263
3113.782489	977981.174487	40.273280
3116.483422	980010.950512	40.278298
3119.687304	982037.779916	40.283316
3122.814461	984083.375472	40.288333
3126.051012	986125.786084	40.293351
3129.856170	988166.106096	40.298368
3133.194412	990197.990824	40.303386
3136.162664	992243.794474	40.308404
3139.578485	994302.977674	40.313421
3142.647884	996360.207935	40.318439
3145.414039	998401.785383	40.323456
3148.577843	1000469.260149	40.328474
3151.404023	1002544.187545	40.333492
3154.935507	1004616.103157	40.338509
3157.963524	1006699.658033	40.343527
3160.822469	1008765.409771	40.348544
3163.925366	1010841.605754	40.353562
3167.040116	1012938.733657	40.358580
3170.326463	1015024.109506	40.363597
3173.324317	1017131.313457	40.368615
3176.375561	1019229.396538	40.373632
3180.083734	1021328.618173	40.378650
3182.931040	1023438.411460	40.383668
3186.470962	1025519.073044	40.388685
3189.621787	1027627.430438	40.393703
3192.277583	1029734.108267	40.398720
3195.666807	1031839.098154	40.403738
3198.524142	1033957.857473	40.408756
3201.819224	1036054.708430	40.413773
3204.877914	1038187.164437	40.418791
3207.716988	1040311.223598	40.423808
3211.454099	1042418.808742	40.428826
3214.378409	1044498.371236	40.433844
3217.636056	1046578.158116	40.438861
3220.645629	1048661.055107	40.443879
3223.565020	1050727.980827	40.448896
3226.875429	1052815.902378	40.453914
3229.724536	1054900.034011	40.458932
3233.123752	1056991.168677	40.463949
3236.610571	1059079.382035	40.468967
3239.463573	1061181.505143	40.473984
3242.614204	1063283.640004	40.479002
3245.849538	1065400.598469	40.484020
3249.585468	1067511.094645	40.489037
3252.887357	1069625.932159	40.494055
3255.553810	1071771.017443	40.499072
3258.633194	1073897.181544	40.504090
3261.670878	1076039.765238	40.509108
3264.911930	1078180.613449	40.514125
3267.989533	1080352.612159	40.519143
3270.951340	1082518.407587	40.524160
3274.239467	1084708.627885	40.529178
3277.371162	1086906.977004	40.534196
3280.634553	1089104.701791	40.539213
3283.802078	1091315.878546	40.544231
3286.946799	1093522.338789	40.549248
3290.087631	1095743.646591	40.554266
3293.497354	1097980.023571	40.559284
3296.640702	1100204.363352	40.564301
3299.886994	1102443.972563	40.569319
3303.377840	1104685.374426	40.574336
3306.942967	1106931.735902	40.579354
3310.280891	1109197.282363	40.584372
3313.606993	1111448.650240	40.589389
3317.014658	1113723.599291	40.594407
3320.447390	1115977.044426	40.599424
3323.627905	1118226.257431	40.604442
3326.917182	1120495.975157	40.609460
3330.103994	1122779.653339	40.614477
3333.606209	1125082.044093	40.619495
3336.941601	1127370.092424	40.624512
3340.216270	1129655.461525	40.629530
3342.974172	1131954.342054	40.634548
3346.316543	1134259.048864	40.639565
3349.218959	1136563.869819	40.644583
3352.723063	1138889.552060	40.649600
3356.228210	1141217.430551	40.654618
3359.627712	1143533.426117	40.659636
3362.829032	1145864.605728	40.664653
3366.143660	1148201.635872	40.669671
3369.298508	1150544.552091	40.674688
3373.101330	1152876.501061	40.679706
3376.583458	1155222.757427	40.684724
3379.898904	1157558.938657	40.689741
3383.655499	1159900.230698	40.694759
3386.952852	1162242.343814	40.699776
3390.625419	1164582.217654	40.704794
3393.392363	1166922.230074	40.709812
3396.986792	1169268.682129	40.714829
3400.293977	1171632.471312	40.719847
3403.523039	1173985.986784	40.724864
3407.133538	1176333.112606	40.729882
3410.179678	1178697.028319	40.734900
3413.630609	1181049.190899	40.739917
3416.920216	1183421.902119	40.744935
3419.828783	1185802.971942	40.749952
3423.644301	1188170.137958	40.754970
3426.813560	1190541.107224	40.759988
3430.268638	1192913.658203	40.765005
3433.614237	1195273.840541	40.770010
3437.022414	1197585.533151	40.775015
3440.034944	1199831.341976	40.780020
3443.286407	1202028.593331	40.785024
3446.589052	1204130.142333	40.790029
3449.865299	1206173.405325	40.795034
3452.632067	1208133.151105	40.800039
3455.541996	1210010.209616	40.805044
3458.029921	1211818.988617	40.810048
3460.742888	1213558.704833	40.815053
3463.209174	1215220.901826	40.820058
3465.650484	1216796.082037	40.825063
3468.570023	1218296.393052	40.830068
3470.353552	1219744.124238	40.835072
3473.039375	1221101.526048	40.840077
3474.914335	1222389.591499	40.845082
3477.015851	1223610.536393	40.850087
3479.094010	1224765.850164	40.855092
3480.797574	1225877.380025	40.860096
3482.782480	1226913.695829	40.865101
3484.698128	1227882.270999	40.870106
3486.257128	1228801.099683	40.875111
3487.948835	1229670.035013	40.880116
3489.746891	1230471.111511	40.885120
3491.096146	1231224.310050	40.890125
3492.665207	1231929.448650	40.895130
3494.094094	1232595.087961	40.900135
3495.515378	1233201.279048	40.905140
3496.706085	1233761.963805	40.910144
3498.084291	1234293.113792	40.915149
3499.353979	1234780.626578	40.920154
3500.039725	1235212.948958	40.925159
3501.403940	1235614.198304	40.930164
3502.155571	1235977.795465	40.935168
3502.896170	1236312.310886	40.940173
3504.128538	1236623.162041	40.945178
3504.829323	1236887.800052	40.950183
3505.785643	1237130.406357	40.955188
3506.690450	1237348.334399	40.960192
3507.299976	1237540.882641	40.965197
3508.283459	1237693.605276	40.970202
3508.553686	1237841.413095	40.975207
3509.452686	1237951.685945	40.980212
3510.045180	1238043.107417	40.985216
3510.583213	1238108.747662	40.990221
3511.061419	1238161.642403	40.995226
3511.603033	1238192.741238	41.000231
3512.169075	1238197.954683	41.005236
3512.586332	1238187.459057	41.010240
3513.206493	1238170.226906	41.015245
3513.562381	1238124.456801	41.020250
3513.947620	1238059.409673	41.025255
3514.431553	1237991.738604	41.030260
3514.837233	1237908.810595	41.035264
3515.284253	1237812.653511	41.040269
3515.504103	1237694.558739	41.045274
3515.709540	1237574.415169	41.050279
3515.980686	1237426.696778	41.055284
3516.309984	1237286.413676	41.060288
3516.539349	1237134.596565	41.065293
3516.793113	1236978.859812	41.070298
3517.036998	1236807.661381	41.075303
3517.519015	1236611.366758	41.080308
3517.850903	1236415.461754	41.085312
3517.711685	1236217.764044	41.090317
3518.164246	1235994.441211	41.095322
3518.142488	1235804.624757	41.100327
3518.173448	1235583.029722	41.105332
3518.430253	1235343.502877	41.110336
3518.549562	1235109.110844	41.115341
3518.846989	1234870.859070	41.120346
3518.656518	1234626.807093	41.125351
3518.980050	1234369.615086	41.130356
3519.121064	1234128.186322	41.135360
3519.031618	1233877.652575	41.140365
3519.460238	1233594.407181	41.145370
3519.236543	1233332.966133	41.150375
3519.676301	1233055.093580	41.155380
3519.624422	1232795.739889	41.160384
3520.032768	1232506.565452	41.165389
3519.939935	1232216.338526	41.170394
3520.127146	1231928.472379	41.175399
3520.143053	1231632.508016	41.180404
3520.315903	1231342.187186	41.185408
3520.182076	1231033.254225	41.190413
3520.422030	1230727.970277	41.195418
3520.206105	1230424.328101	41.200423
3520.661873	1230118.598906	41.205428
3520.559038	1229807.534603	41.210432
3520.648467	1229497.352112	41.215437
3520.680781	1229175.875067	41.220442
3520.296246	1228853.513569	41.225447
3520.655486	1228535.672869	41.230452
3520.684244	1228223.183734	41.235456
3520.524470	1227888.783755	41.240461
3521.011182	1227577.392137	41.245466
3520.930402	1227251.893327	41.250471
3520.860599	1226909.763375	41.255476
3520.785012	1226593.738667	41.260480
3520.896849	1226258.439937	41.265485
3520.929241	1225911.653251	41.270490
3520.773585	1225580.833363	41.275495
3520.886667	1225242.014040	41.280500
3520.870128	1224913.087787	41.285504
3520.934344	1224581.233111	41.290509
3521.042561	1224238.333610	41.295514
3520.360648	1223897.034865	41.300519
3520.783344	1223548.155208	41.305524
3520.954724	1223234.214824	41.310528
3520.886060	1222892.000562	41.315533
3521.166878	1222542.795120	41.320538
3521.079916	1222196.895004	41.325543
3521.311308	1221846.342370	41.330548
3521.285562	1221506.829759	41.335552
3521.006464	1221157.901630	41.340557
3521.164285	1220800.376549	41.345562
3520.687729	1220444.051917	41.350567
3521.104220	1220084.285150	41.355572
3520.975690	1219740.840908	41.360576
3520.643915	1219384.044448	41.365581
3520.691551	1219020.058223	41.370586
3520.878262	1218693.032165	41.375591
3520.971254	1218339.830852	41.380596
3520.985187	1217992.226262	41.385600
3521.019191	1217640.388219	41.390605
3521.142929	1217284.771795	41.395610
3520.847462	1216928.264704	41.400615
3520.872629	1216576.728642	41.405620
3520.384431	1216228.244957	41.410624
3520.460198	1215874.969137	41.415629
3520.547364	1215526.997330	41.420634
3520.274376	1215187.478018	41.425639
3520.382460	1214841.513478	41.430644
3520.680673	1214488.198520	41.435648
3520.645701	1214131.920682	41.440653
3520.685900	1213778.224916	41.445658
3520.409510	1213429.795782	41.450663
3520.639421	1213073.306894	41.455668
3520.366701	1212729.133102	41.460672
3520.569371	1212373.348384	41.465677
3521.054319	1212020.767681	41.470682
3520.180224	1211674.282376	41.475687
3520.547781	1211320.924044	41.480692
3520.275490	1210966.617085	41.485696
3520.362581	1210607.639732	41.490701
3520.666840	1210262.830375	41.495706
3520.401540	1209908.729794	41.500711
3520.743327	1209551.883232	41.505716
3520.751172	1209185.703679	41.510720
3520.661866	1208834.215043	41.515725
3520.793547	1208473.114176	41.520730
3520.383243	1208113.950114	41.525735
3520.632174	1207743.038758	41.530740
3520.171914	1207394.134742	41.535744
3519.873304	1207042.744899	41.540749
3520.345908	1206685.302297	41.545754
3520.171067	1206340.401275	41.550759
3520.619047	1205986.567646	41.555764
3520.258234	1205622.442519	41.560768
3520.396889	1205256.991126	41.565773
3520.304659	1204899.798156	41.570778
3520.009111	1204558.826640	41.575783
3520.395190	1204187.541630	41.580788
3519.928930	1203837.271721	41.585792
3520.159848	1203491.362368	41.590797
3520.403521	1203130.053966	41.595802
3520.031895	1202782.321226	41.600807
3519.979710	1202405.354570	41.605812
3519.774284	1202071.140751	41.610816
3519.706014	1201717.566494	41.615821
3519.546019	1201359.669394	41.620826
3519.373203	1201018.254845	41.625831
3519.598865	1200678.346356	41.630836
3519.698375	1200333.277559	41.635840
3519.734335	1199980.129328	41.640845
3519.760633	1199636.714223	41.645850
3519.610996	1199284.393022	41.650855
3519.866876	1198930.761257	41.655860
3519.736127	1198576.324435	41.660864
3519.450898	1198233.148389	41.665869
3519.571392	1197891.947055	41.670874
3519.172645	1197545.084150	41.675879
3519.435013	1197182.603699	41.680884
3519.460380	1196841.911533	41.685888
3519.487967	1196495.564691	41.690893
3519.535831	1196140.742984	41.695898
3519.192655	1195797.038569	41.700903
3519.479640	1195452.550263	41.705908
3519.543102	1195096.996930	41.710912
3519.316943	1194747.757716	41.715917
3519.036332	1194393.996548	41.720922
3519.206470	1194055.443784	41.725927
3519.265952	1193701.015614	41.730932
3519.492865	1193358.557290	41.735936
3519.112569	1193008.943908	41.740941
3519.172150	1192657.637525	41.745946
3518.773044	1192325.076629	41.750951
3518.942235	1191964.405049	41.755956
3519.007419	1191649.103999	41.760960
3519.051588	1191303.157122	41.765965
3518.939808	1190954.017983	41.770970
3518.900189	1190617.247398	41.775975
3518.845128	1190280.645349	41.780980
3518.882847	1189952.652439	41.785984
3518.821294	1189593.826914	41.790989
3518.845993	1189248.591532	41.795994
3518.526615	1188920.215924	41.800999
3518.482243	1188574.946925	41.806004
3518.309317	1188243.213942	41.811008
3518.185435	1187916.998724	41.816013
3518.541695	1187584.666254	41.821018
3518.402535	1187251.829846	41.826023
3518.595592	1186906.034205	41.831028
3518.584091	1186571.158204	41.836032
3518.395005	1186236.760029	41.841037
3518.497344	1185899.846808	41.846042
3518.094854	1185563.276990	41.851047
3518.390302	1185241.621187	41.856052
3518.102985	1184901.320734	41.861056
3518.281921	1184570.705442	41.866061
3518.246462	1184227.967280	41.871066
3518.041849	1183905.652284	41.876071
3518.018179	1183568.608172	41.881076
3518.340846	1183248.894338	41.886080
3517.867644	1182912.822659	41.891085
3518.008209	1182579.169237	41.896090
3517.832696	1182256.276306	41.901095
3518.192400	1181923.956477	41.906100
3518.100762	1181594.043045	41.911104
3517.494652	1181263.722662	41.916109
3517.764918	1180928.529618	41.921114
3517.627986	1180628.971323	41.926119
3517.722791	1180292.353830	41.931124
3517.646435	1179974.292889	41.936128
3517.568090	1179643.217456	41.941133
3517.656129	1179310.963413	41.946138
3517.562684	1178982.485257	41.951143
3517.505000	1178661.327034	41.956148
3517.357885	1178343.177858	41.961152
3517.050397	1178020.702480	41.966157
3517.327825	1177705.081885	41.971162
3517.326002	1177377.146590	41.976167
3517.200628	1177052.885392	41.981172
3517.316655	1176733.840647	41.986176
3517.226447	1176426.306067	41.991181
3517.242080	1176109.218324	41.996186
3517.138561	1175786.193818	42.001191
3517.281292	1175467.255480	42.006196
3517.352843	1175153.116103	42.011200
3517.056276	1174826.859322	42.016205
3517.066374	1174512.597156	42.021210
3516.790385	1174196.383514	42.026215
3517.170365	1173883.059388	42.031220
3517.074884	1173578.939803	42.036224
3516.791166	1173250.885126	42.041229
3516.624791	1172936.085468	42.046234
3516.517864	1172628.046335	42.051239
3516.695189	1172317.867539	42.056244
3516.668064	1172029.583252	42.061248
3516.666130	1171703.459500	42.066253
3516.902940	1171397.365918	42.071258
3516.728175	1171084.813791	42.076263
3516.881284	1170774.358520	42.081268
3516.451318	1170471.621964	42.086272
3516.628957	1170169.145131	42.091277
3516.760079	1169833.448457	42.096282
3516.545726	1169522.979247	42.101287
3516.365756	1169216.354582	42.106292
3516.441409	1168907.782535	42.111296
3516.244589	1168596.594791	42.116301
3516.687850	1168290.756819	42.121306
3516.307390	1167989.566855	42.126311
3516.396899	1167677.994081	42.131316
3516.187387	1167376.551841	42.136320
3516.167326	1167073.645058	42.141325
3516.037291	1166773.476491	42.146330
3515.637476	1166474.468004	42.151335
3515.909092	1166173.537983	42.156340
3516.021046	1165883.569461	42.161344
3516.046987	1165578.680108	42.166349
3516.156107	1165286.790494	42.171354
3516.032684	1164981.513215	42.176359
3515.983709	1164675.639220	42.181364
3515.884840	1164382.883467	42.186368
3515.765668	1164083.597587	42.191373
3515.943543	1163782.073181	42.196378
3515.630382	1163490.152885	42.201383
3515.921650	1163195.755096	42.206388
3515.941859	1162900.535154	42.211392
3515.476365	1162598.009324	42.216397
3515.801561	1162299.965452	42.221402
3515.197561	1162014.624577	42.226407
3515.710147	1161715.288244	42.231412
3515.733857	1161421.307263	42.236416
3515.354364	1161135.031012	42.241421
3515.754395	1160843.979795	42.246426
3515.435695	1160548.683133	42.251431
3515.554378	1160256.700511	42.256436
3515.489052	1159972.010353	42.261440
3515.030130	1159672.622870	42.266445
3515.376263	1159373.274775	42.271450
3515.442405	1159100.710751	42.276455
3515.363585	1158815.203704	42.281460
3515.492580	1158526.243066	42.286464
3515.044491	1158241.522027	42.291469
3515.259945	1157943.248561	42.296474
3515.062637	1157672.734109	42.301479
3515.207286	1157375.101993	42.306484
3515.284163	1157083.327940	42.311488
3515.059122	1156797.262326	42.316493
3515.011719	1156512.570679	42.321498
3515.175202	1156229.909903	42.326503
3515.113713	1155938.757210	42.331508
3514.903594	1155651.018558	42.336512
3514.775850	1155366.372640	42.341517
3514.663181	1155084.074145	42.346522
3515.011042	1154817.107341	42.351527
3514.936938	1154520.863443	42.356532
3515.102219	1154238.095260	42.361536
3514.665266	1153969.227481	42.366541
3515.013799	1153684.885254	42.371546
3514.745711	1153393.720263	42.376551
3514.705084	1153117.740079	42.381556
3514.701786	1152842.117885	42.386560
3514.563345	1152561.581290	42.391565
3514.935638	1152274.603184	42.396570
3514.645878	1151999.268024	42.401575
3514.430840	1151716.048267	42.406580
3514.352874	1151441.690472	42.411584
3514.264242	1151174.989480	42.416589
3514.339293	1150896.127955	42.421594
3514.127403	1150631.692269	42.426599
3514.676676	1150360.489110	42.431604
3514.414231	1150084.007632	42.436608
3514.214173	1149806.554292	42.441613
3514.020526	1149544.902289	42.446618
3514.118905	1149274.854087	42.451623
3514.133595	1148999.785561	42.456628
3514.005494	1148737.609083	42.461632
3514.085629	1148465.438442	42.466637
3514.222754	1148185.097007	42.471642
3513.914721	1147927.646738	42.476647
3513.772223	1147668.640701	42.481652
3514.399462	1147398.693577	42.486656
3513.731859	1147122.123480	42.491661
3513.948306	1146861.597375	42.496666
3513.739739	1146606.530032	42.501671
3513.738638	1146327.913234	42.506676
3513.281732	1146079.495232	42.511680
3513.304726	1145832.408186	42.516685
3513.840163	1145556.316129	42.521690
3513.579101	1145299.014227	42.526695
3513.660435	1145039.747532	42.531700
3513.571470	1144782.392122	42.536704
3513.389582	1144524.849874	42.541709
3513.474083	1144259.477006	42.546714
3513.510217	1144008.510197	42.551719
3513.571877	1143749.941958	42.556724
3513.422700	1143504.006987	42.561728
3513.382538	1143238.129274	42.566733
3513.703606	1142980.997920	42.571738
3512.938627	1142731.619717	42.576743
3513.289578	1142476.640122	42.581748
3513.397166	1142219.791445	42.586752
3513.140745	1141972.475091	42.591757
3513.169075	1141713.053963	42.596762
3512.952458	1141462.671925	42.601767
3513.263684	1141214.562655	42.606772
3513.467426	1140957.257418	42.611776
3513.104656	1140714.073887	42.616781
3513.520012	1140452.440077	42.621786
3512.940713	1140199.116853	42.626791
3512.829342	1139940.390896	42.631796
3513.248727	1139704.053622	42.636800
3512.944154	1139452.831892	42.641805
3513.014730	1139205.617072	42.646810
3512.910370	1138961.456402	42.651815
3512.691522	1138708.571918	42.656820
3512.988444	1138461.854563	42.661824
3512.758535	1138218.534541	42.666829
3512.888352	1137960.716253	42.671834
3512.889162	1137717.809850	42.676839
3512.760532	1137462.667795	42.681844
3512.780769	1137221.728978	42.686848
3512.537478	1136978.733986	42.691853
3512.780693	1136731.944990	42.696858
3512.777105	1136500.281653	42.701863
3512.607822	1136249.170604	42.706868
3512.788949	1136010.429092	42.711872
3512.497425	1135767.576470	42.716877
3512.666957	1135524.161979	42.721882
3512.428442	1135286.691554	42.726887
3512.059566	1135040.019650	42.731892
3512.465746	1134802.421383	42.736896
3512.406318	1134571.632817	42.741901
3512.586973	1134326.736886	42.746906
3512.212054	1134088.570433	42.751911
3512.335106	1133846.891507	42.756916
3512.174073	1133616.648137	42.761920
3512.238977	1133377.047369	42.766925
3512.068649	1133140.609752	42.771930
3512.202945	1132911.332249	42.776935
3512.100521	1132671.442193	42.781940
3511.794965	1132432.524955	42.786945
3511.873389	1132209.402614	42.791949
3512.057087	1131986.063518	42.796954
3511.666341	1131763.379836	42.801959
3511.856657	1131519.873451	42.806964
3511.969002	1131296.707229	42.811969
3511.655073	1131074.077065	42.816973
3512.005997	1130850.852847	42.821978
3512.171978	1130609.875096	42.826983
3511.842380	1130383.511594	42.831988
3512.322095	1130151.586762	42.836993
3511.846667	1129938.156452	42.841997
3512.108898	1129691.987849	42.847002
3511.718709	1129458.655007	42.852007
3512.013433	1129234.231382	42.857012
3512.198864	1129009.245819	42.862017
3511.965115	1128776.998296	42.867021
3512.109204	1128529.939670	42.872026
3512.118598	1128294.968594	42.877031
3511.597243	1128075.575383	42.882036
3511.539760	1127845.445430	42.887041
3511.956757	1127623.501531	42.892045
3511.892336	1127394.399397	42.897050
3511.496700	1127168.670920	42.902055
3511.530261	1126938.296567	42.907060
3511.545885	1126704.681087	42.912065
3511.479070	1126484.767007	42.917069
3511.452764	1126266.930026	42.922074
3511.553511	1126056.103063	42.927079
3511.322054	1125827.912432	42.932084
3511.432783	1125608.503792	42.937089
3511.228056	1125395.417638	42.942093
3511.362396	1125172.942563	42.947098
3510.913596	1124949.602724	42.952103
3511.067886	1124723.394661	42.957108
3510.949480	1124523.105584	42.962113
3511.065616	1124321.342903	42.967117
3510.979372	1124099.144878	42.972122
3511.060885	1123879.194096	42.977127
3510.799205	1123674.233338	42.982132
3510.999054	1123470.901919	42.987137
3510.785393	1123259.254781	42.992141
3511.211111	1123037.499348	42.997146
3510.914210	1122826.705455	43.002151
3510.650375	1122623.703718	43.007156
3511.016765	1122407.453161	43.012161
3510.956310	1122191.644961	43.017165
3510.851201	1121983.642259	43.022170
3510.499160	1121779.861332	43.027175
3510.677366	1121567.130501	43.032180
3510.662392	1121369.086383	43.037185
3510.731910	1121165.022145	43.042189
3510.914728	1120952.170863	43.047194
3510.573704	1120752.634020	43.052199
3510.602536	1120542.839081	43.057204
3510.611320	1120331.039278	43.062209
3510.299463	1120128.522046	43.067213
3510.519491	1119928.957293	43.072218
3510.460712	1119727.621346	43.077223
3510.784956	1119513.737062	43.082228
3510.716359	1119316.482987	43.087233
3510.702532	1119129.786088	43.092237
3511.367474	1118917.441222	43.097242
3510.764135	1118698.342546	43.102247
3510.899504	1118474.635634	43.107252
3510.586838	1118269.094817	43.112257
3510.504563	1118070.653808	43.117261
3510.679221	1117867.875579	43.122266
3510.577616	1117657.512570	43.127271
3510.525174	1117444.941612	43.132276
3510.633688	1117242.627033	43.137281
3510.345831	1117053.139415	43.142285
3510.457243	1116837.277376	43.147290
3510.305348	1116644.894004	43.152295
3510.444178	1116441.781779	43.157300
3510.444466	1116249.073217	43.162305
3510.205322	1116055.444045	43.167309
3510.121922	1115836.142553	43.172314
3510.053531	1115649.047302	43.177319
3510.095794	1115460.116184	43.182324
3510.158195	1115259.640748	43.187329
3510.226583	1115056.964266	43.192333
3510.411958	1114853.974859	43.197338
3510.219897	1114668.486402	43.202343
3510.482416	1114467.662390	43.207348
3510.548287	1114265.528447	43.212353
3510.215606	1114068.410542	43.217357
3510.207591	1113864.080669	43.222362
3510.065846	1113676.928673	43.227367
3509.922195	1113473.369082	43.232372
3510.094794	1113280.906862	43.237377
3509.932167	1113094.977688	43.242381
3509.508099	1112889.153382	43.247386
3509.368053	1112712.839341	43.252391
3509.325031	1112527.538397	43.257396
3509.608022	1112344.752544	43.262401
3509.614058	1112151.514241	43.267405
3509.611221	1111969.430351	43.272410
3509.421588	1111794.334293	43.277415
3509.486159	1111611.177896	43.282420
3509.682323	1111421.602223	43.287425
3509.016496	1111242.273880	43.292429
3509.227007	1111041.425610	43.297434
3509.022265	1110879.085805	43.302439
3509.403365	1110696.132284	43.307444
3509.464057	1110511.984982	43.312449
3509.482728	1110333.944710	43.317453
3509.480940	1110147.982382	43.322458
3509.747134	1109979.526618	43.327463
3509.415824	1109784.922856	43.332468
3509.730402	1109605.950932	43.337473
3509.336915	1109428.043955	43.342477
3509.379586	1109233.263194	43.347482
3509.548274	1109063.076993	43.352487
3509.180203	1108883.620842	43.357492
3509.332756	1108703.213979	43.362497
3509.399754	1108518.997358	43.367501
3509.284287	1108329.650271	43.372506
3509.256485	1108150.399950	43.377511
3509.237865	1107965.414858	43.382516
3509.135518	1107791.510321	43.387521
3508.786526	1107617.163478	43.392525
3509.175948	1107446.126075	43.397530
3509.104430	1107271.626872	43.402535
3508.832410	1107098.396144	43.407540
3509.038841	1106909.614348	43.412545
3508.920044	1106758.019876	43.417549
3509.299466	1106582.182861	43.422554
3509.073378	1106411.309433	43.427559
3509.028756	1106242.501373	43.432564
3508.985425	1106058.982578	43.437569
3509.058504	1105882.886717	43.442573
3508.762232	1105706.177465	43.447578
3508.850063	1105540.763404	43.452583
3508.733409	1105361.721317	43.457588
3508.445141	1105191.201405	43.462593
3508.803319	1105041.008093	43.467597
3508.960685	1104864.100989	43.472602
3509.091079	1104697.316883	43.477607
3508.861406	1104519.125019	43.482612
3508.736125	1104347.596398	43.487617
3508.484545	1104183.629351	43.492621
3508.337415	1104011.520497	43.497626
3508.463391	1103855.027732	43.502631
3508.596862	1103681.620272	43.507636
3508.675158	1103512.993011	43.512641
3508.595937	1103365.213389	43.517645
3508.464783	1103200.623381	43.522650
3508.271516	1103034.318816	43.527655
3508.556790	1102878.153633	43.532660
3508.949867	1102708.111731	43.537665
3508.597354	1102552.519902	43.542669
3508.509730	1102375.284815	43.547674
3508.441148	1102224.796675	43.552679
3508.450168	1102056.804186	43.557684
3508.576521	1101887.640392	43.562689
3508.261839	1101725.424646	43.567693
3508.322034	1101563.620122	43.572698
3508.012872	1101416.589515	43.577703
3508.125888	1101255.531621	43.582708
3508.332658	1101102.864215	43.587713
3508.032360	1100938.806494	43.592717
3508.269071	1100778.383047	43.597722
3508.189128	1100630.719782	43.602727
3508.329337	1100473.266293	43.607732
3508.321404	1100317.553239	43.612737
3508.338362	1100155.522446	43.617741
3508.091521	1099991.905105	43.622746
3507.980258	1099829.885657	43.627751
3507.949781	1099685.438756	43.632756
3507.995984	1099536.003946	43.637761
3508.055813	1099382.929698	43.642765
3508.017345	1099210.362908	43.647770
3507.854545	1099074.430739	43.652775
3507.862543	1098907.009670	43.657780
3508.145482	1098751.107932	43.662785
3508.027098	1098602.821835	43.667789
3508.127976	1098450.670622	43.672794
3508.006516	1098306.393079	43.677799
3507.638442	1098158.040272	43.682804
3508.086951	1098001.133350	43.687809
3507.661792	1097859.475938	43.692813
3507.562426	1097698.729484	43.697818
3507.855533	1097552.928998	43.702823
3507.847781	1097393.019121	43.707828
3507.427996	1097255.648886	43.712833
3507.281403	1097114.786873	43.717837
3507.637640	1096961.308275	43.722842
3507.837347	1096827.842429	43.727847
3507.778716	1096678.632831	43.732852
3508.122826	1096526.196092	43.737857
3507.790450	1096372.814213	43.742861
3507.427687	1096228.520951	43.747866
3507.582239	1096088.252242	43.752871
3507.365424	1095944.884028	43.757876
3507.760663	1095801.315539	43.762881
3507.545290	1095654.782280	43.767885
3507.605160	1095499.684601	43.772890
3508.001121	1095353.712235	43.777895
3507.690371	1095215.315421	43.782900
3507.991210	1095056.816545	43.787905
3507.787457	1094921.456462	43.792909
3507.668817	1094758.520705	43.797914
3507.681807	1094624.744212	43.802919
3507.546391	1094485.917103	43.807924
3507.584639	1094328.588481	43.812929
3507.353810	1094184.218962	43.817933
3507.362084	1094035.021142	43.822938
3507.476529	1093908.100736	43.827943
3507.176319	1093757.989053	43.832948
3507.635531	1093603.824062	43.837953
3507.297752	1093480.222218	43.842957
3507.534143	1093333.360283	43.847962
3507.511896	1093192.471383	43.852967
3507.252336	1093054.680906	43.857972
3507.326260	1092910.993002	43.862977
3507.183178	1092771.357429	43.867981
3507.332850	1092623.437576	43.872986
3507.487199	1092484.128522	43.877991
3507.069385	1092350.653999	43.882996
3507.063636	1092208.970959	43.888001
3506.924665	1092088.942502	43.893005
3507.084073	1091944.257531	43.898010
3507.103701	1091814.814512	43.903015
3507.121952	1091678.953846	43.908020
3507.248542	1091554.561379	43.913025
3507.030428	1091406.956144	43.918029
3507.013919	1091279.612753	43.923034
3507.085363	1091157.997026	43.928039
3507.131858	1091015.316666	43.933044
3507.228156	1090876.646157	43.938049
3507.030236	1090747.500761	43.943053
3507.248416	1090614.166000	43.948058
3507.172379	1090482.504412	43.953063
3507.130703	1090340.970007	43.958068
3507.317307	1090202.171619	43.963073
3506.923573	1090069.498870	43.968077
3507.005120	1089940.096679	43.973082
3506.999343	1089814.153723	43.978087
3506.511640	1089676.698038	43.983092
3507.201690	1089539.044895	43.988097
3506.825172	1089410.375983	43.993101
3507.128605	1089282.933027	43.998106
3507.099048	1089131.211813	44.003111
3506.801387	1089010.279252	44.008116
3506.838429	1088874.728418	44.013121
3507.062774	1088756.578008	44.018125
3506.886975	1088609.943426	44.023130
3506.780605	1088485.327366	44.028135
3506.793500	1088357.910554	44.033140
3506.681242	1088233.385483	44.038145
3506.846581	1088092.141551	44.043149
3506.948354	1087964.796686	44.048154
3506.525628	1087834.852515	44.053159
3506.496126	1087713.463651	44.058164
3506.778025	1087576.786149	44.063169
3506.358534	1087453.060309	44.068173
3506.356951	1087348.235116	44.073178
3506.797307	1087220.337940	44.078183
3506.657204	1087098.761915	44.083188
3506.682540	1086971.789660	44.088193
3506.468665	1086854.724150	44.093197
3506.614601	1086724.563925	44.098202
3506.584523	1086599.796206	44.103207
3506.599313	1086477.030766	44.108212
3506.618708	1086351.865869	44.113217
3506.732065	1086224.957508	44.118221
3506.693058	1086090.499791	44.123226
3506.460651	1085970.447190	44.128231
3506.585323	1085842.090371	44.133236
3506.415281	1085717.804690	44.138241
3505.963024	1085610.048898	44.143245
3506.360995	1085482.597084	44.148250
3506.233286	1085366.443846	44.153255
3506.306950	1085255.527065	44.158260
3506.489223	1085129.827928	44.163265
3506.414788	1085014.712848	44.168269
3506.654531	1084893.504235	44.173274
3506.754317	1084780.943810	44.178279
3506.687670	1084648.468147	44.183284
3506.623142	1084536.984274	44.188289
3506.371626	1084412.202824	44.193293
3506.410057	1084284.686300	44.198298
3506.491467	1084161.378240	44.203303
3506.063923	1084044.958533	44.208308
3506.491698	1083919.766277	44.213313
3506.097162	1083804.678310	44.218317
3506.456638	1083684.861289	44.223322
3506.444349	1083574.020270	44.228327
3506.291785	1083459.556353	44.233332
3506.496252	1083332.277832	44.238337
3506.152309	1083221.963717	44.243341
3506.465959	1083091.784825	44.248346
3506.549836	1082980.436410	44.253351
3506.639203	1082850.959977	44.258356
3506.497236	1082728.615240	44.263361
3506.023610	1082625.119345	44.268365
3506.266798	1082508.172672	44.273370
3506.097156	1082392.442364	44.278375
3505.887103	1082265.015356	44.283380
3506.243236	1082152.550173	44.288385
3506.142433	1082043.706708	44.293389
3505.748583	1081933.470608	44.298394
3506.152321	1081812.645966	44.303399
3506.060110	1081706.480023	44.308404
3506.127606	1081591.173225	44.313409
3505.905180	1081481.187498	44.318413
3506.345953	1081376.845809	44.323418
3506.339740	1081237.178728	44.328423
3506.140009	1081134.664582	44.333428
3505.955260	1081009.122602	44.338433
3505.583611	1080907.112143	44.343437
3505.812716	1080790.898398	44.348442
3505.910217	1080683.434118	44.353447
3505.699744	1080583.789482	44.358452
3506.054257	1080477.046315	44.363457
3505.998649	1080357.608248	44.368461
3505.655798	1080250.879565	44.373466
3506.108532	1080145.744796	44.378471
3505.706942	1080028.275422	44.383476
3505.850152	1079913.688252	44.388481
3505.901474	1079816.673086	44.393485
3505.855855	1079696.163408	44.398490
3505.846079	1079598.194875	44.403495
3505.866076	1079497.628819	44.408500
3506.040385	1079371.894031	44.413505
3505.893046	1079279.604069	44.418509
3505.477272	1079161.062761	44.423514
3505.591215	1079064.983547	44.428519
3505.481173	1078956.079926	44.433524
3505.377049	1078838.535917	44.438529
3505.450341	1078743.225488	44.443533
3505.536998	1078643.688390	44.448538
3505.603035	1078543.673000	44.453543
3505.773773	1078441.335101	44.458548
3506.132349	1078334.645328	44.463553
3505.681829	1078237.684731	44.468557
3505.490993	1078138.376079	44.473562
3505.734786	1078029.011749	44.478567
3505.549819	1077920.483729	44.483572
3505.882159	1077806.781014	44.488577
3505.598558	1077713.623108	44.493581
3505.676622	1077607.157297	44.498586
3505.760280	1077505.296148	44.503591
3505.465408	1077402.727484	44.508596
3505.625524	1077284.434513	44.513601
3505.414824	1077191.351680	44.518605
3505.331163	1077079.430305	44.523610
3505.449036	1076978.705699	44.528615
3505.197104	1076889.560594	44.533620
3505.413957	1076780.463706	44.538625
3505.532360	1076695.286668	44.543629
3505.512339	1076589.297201	44.548634
3505.545289	1076502.787110	44.553639
3505.415006	1076394.795808	44.558644
3505.541476	1076287.912254	44.563649
3505.505281	1076190.078907	44.568653
3505.681886	1076087.023803	44.573658
3505.690793	1075988.219235	44.578663
3505.249532	1075887.374555	44.583668
3505.760690	1075787.235356	44.588673
3505.299947	1075703.482562	44.593677
3505.381482	1075600.914070	44.598682
3505.609909	1075495.534645	44.603687
3505.370042	1075403.482442	44.608692
3505.414746	1075288.046139	44.613697
3505.516154	1075195.261997	44.618701
3505.303237	1075081.016152	44.623706
3505.117594	1074991.829143	44.628711
3504.961716	1074903.980316	44.633716
3505.493736	1074794.791877	44.638721
3505.114244	1074699.773556	44.643725
3505.432279	1074600.220682	44.648730
3505.125720	1074517.000557	44.653735
3504.958553	1074422.710809	44.658740
3505.184321	1074323.648332	44.663745
3505.253434	1074225.186166	44.668749
3505.316369	1074132.486374	44.673754
3505.213864	1074041.925440	44.678759
3504.963552	1073934.961869	44.683764
3505.353347	1073850.944523	44.688769
3505.138793	1073775.478567	44.693773
3504.936079	1073674.553736	44.698778
3505.098999	1073584.709995	44.703783
3504.920151	1073490.790344	44.708788
3505.172271	1073401.505284	44.713793
3505.032492	1073305.942919	44.718797
3505.032720	1073204.591724	44.723802
3504.987866	1073125.438244	44.728807
3505.091561	1073035.403098	44.733812
3505.302378	1072940.353031	44.738817
3504.976690	1072857.014705	44.743821
3504.835198	1072771.242870	44.748826
3504.994748	1072677.349591	44.753831
3504.971971	1072585.022000	44.758836
3505.040613	1072491.524823	44.763841
3504.967476	1072411.404861	44.768845
3504.936928	1072314.173778	44.773850
3505.128165	1072224.591295	44.778855
3504.707762	1072134.339384	44.783860
3505.430086	1072036.018492	44.788865
3504.803936	1071956.655574	44.793869
3504.901305	1071862.470287	44.798874
3504.918648	1071772.140305	44.803879
3504.572520	1071689.364111	44.808884
3505.014467	1071602.516913	44.813889
3504.853458	1071512.308114	44.818893
3504.761771	1071437.077943	44.823898
3504.896245	1071339.321866	44.828903
3504.419631	1071247.911373	44.833908
3504.584111	1071155.048302	44.838913
3504.552604	1071089.029451	44.843917
3504.896667	1071011.511237	44.848922
3504.809389	1070931.564153	44.853927
3504.792754	1070844.972693	44.858932
3505.013017	1070752.285827	44.863937
3504.788676	1070669.089695	44.868941
3504.675140	1070578.569350	44.873946
3504.928257	1070496.925911	44.878951
3504.405424	1070404.259428	44.883956
3504.766743	1070314.329330	44.888961
3504.540636	1070248.524635	44.893965
3504.734753	1070164.386831	44.898970
3504.693520	1070076.153196	44.903975
3504.391986	1069984.019889	44.908980
3504.348807	1069917.700464	44.913985
3504.577646	1069848.643872	44.918989
3504.544999	1069761.461154	44.923994
3504.705069	1069681.166692	44.928999
3504.258815	1069606.546548	44.934004
3504.698165	1069522.646897	44.939009
3504.500973	1069442.792315	44.944013
3504.816276	1069355.545833	44.949018
3504.837813	1069271.615020	44.954023
3504.469201	1069187.266484	44.959028
3504.606014	1069102.641125	44.964033
3504.906876	1069032.697130	44.969037
3504.533428	1068941.615690	44.974042
3505.014267	1068863.852294	44.979047
3504.604473	1068787.292088	44.984052
3504.480559	1068698.761451	44.989057
3504.366273	1068614.939100	44.994061
3504.564672	1068536.736840	44.999066
3504.764125	1068446.802771	45.004071
3504.535734	1068363.860741	45.009076
3504.660012	1068283.840168	45.014081
3504.444766	1068210.412964	45.019085
3504.471418	1068120.694320	45.024090
3504.523858	1068032.123871	45.029095
3504.287133	1067966.389664	45.034100
3504.476626	1067898.084270	45.039105
3504.431965	1067824.527639	45.044109
3504.100332	1067740.727716	45.049114
3504.490727	1067660.365726	45.054119
3504.305821	1067600.484700	45.059124
3504.644807	1067502.530323	45.064129
3504.411362	1067441.309194	45.069133
3504.178031	1067356.044657	45.074138
3504.579641	1067274.713464	45.079143
3504.175286	1067191.878852	45.084148
3504.381647	1067123.849565	45.089153
3504.420183	1067047.191202	45.094157
3504.197940	1066975.864494	45.099162
3504.367685	1066900.528960	45.104167
3504.476779	1066830.107576	45.109172
3504.359795	1066743.179283	45.114177
3504.608680	1066676.772542	45.119181
3504.432011	1066584.465317	45.124186
3504.453335	1066501.838725	45.129191
3504.173657	1066441.672094	45.134196
3504.190335	1066360.198378	45.139201
3503.959301	1066287.806096	45.144205
3504.043373	1066219.978127	45.149210
3504.224755	1066145.976994	45.154215
3503.923916	1066075.036284	45.159220
3504.462356	1065996.645623	45.164225
3504.112393	1065942.256777	45.169229
3504.275644	1065878.066984	45.174234
3504.004813	1065785.858028	45.179239
3503.834170	1065714.506418	45.184244
3503.707241	1065645.263102	45.189249
3503.860618	1065575.106927	45.194253
3504.272397	1065512.699774	45.199258
3504.465111	1065434.935261	45.204263
3503.808416	1065365.583261	45.209268
3503.942790	1065286.286957	45.214273
3503.888551	1065229.533361	45.219277
3503.950021	1065152.459922	45.224282
3504.165651	1065095.564286	45.229287
3504.009082	1065022.180933	45.234292
3504.034951	1064954.250703	45.239297
3504.124303	1064889.869106	45.244301
3504.133629	1064821.170240	45.249306
3504.132456	1064750.066828	45.254311
3503.854918	1064673.908458	45.259316
3503.944922	1064601.344833	45.264321
3504.126247	1064550.318576	45.269325
3503.955605	1064469.809859	45.274330
3504.128823	1064399.346735	45.279335
3503.911632	1064334.431779	45.284340
3504.265616	1064256.912702	45.289345
3504.011882	1064198.641703	45.294349
3504.009678	1064117.330266	45.299354
3504.371863	1064046.350356	45.304359
3504.078950	1063987.602425	45.309364
3504.224167	1063909.535454	45.314369
3503.882667	1063843.961553	45.319373
3503.792321	1063774.881087	45.324378
3504.388922	1063716.272452	45.329383
3503.904841	1063652.548209	45.334388
3504.071686	1063565.907791	45.339393
3503.733745	1063499.848006	45.344397
3503.896426	1063446.986044	45.349402
3503.984360	1063370.364442	45.354407
3504.012273	1063304.242049	45.359412
3503.823457	1063234.593556	45.364417
3503.736160	1063173.974432	45.369421
3503.923315	1063107.245976	45.374426
3503.888421	1063039.494568	45.379431
3503.532402	1062980.553761	45.384436
3503.731866	1062905.639771	45.389441
3503.641140	1062851.851334	45.394445
3503.635793	1062783.803158	45.399450
3504.000127	1062724.933469	45.404455
3503.420689	1062667.373628	45.409460
3503.672896	1062593.312976	45.414465
3503.507654	1062543.865246	45.419469
3503.505304	1062480.433076	45.424474
3503.720816	1062412.921473	45.429479
3503.879672	1062354.081659	45.434484
3503.861549	1062299.505790	45.439489
3503.708989	1062233.785283	45.444493
3503.389480	1062173.482151	45.449498
3503.625463	1062103.075519	45.454503
3503.414782	1062056.422515	45.459508
3503.654129	1061987.457807	45.464513
3503.671541	1061940.188659	45.469517
3503.868029	1061887.113605	45.474522
3503.887368	1061805.860689	45.479527
3503.602516	1061758.447225	45.484532
3503.921681	1061682.341632	45.489537
3503.925251	1061622.364323	45.494541
3503.717107	1061564.346680	45.499546
3503.552006	1061503.240582	45.504551
3503.540669	1061448.847699	45.509556
3503.566799	1061375.289259	45.514561
3503.898613	1061335.280086	45.519565
3503.687986	1061254.538284	45.524570
3503.787144	1061186.741967	45.529575
3503.686385	1061135.730483	45.534580
3503.931835	1061065.694141	45.539585
3503.896238	1061009.471567	45.544589
3503.986080	1060940.422081	45.549594
3503.970204	1060881.787869	45.554599
3503.489327	1060814.852776	45.559604
3503.942001	1060740.830461	45.564609
3503.521041	1060689.386140	45.569613
3503.336724	1060628.947506	45.574618
3503.732813	1060569.375514	45.579623
3503.601753	1060516.533771	45.584628
3503.942933	1060453.503099	45.589633
3503.870894	1060391.021229	45.594637
3503.777954	1060333.067914	45.599642
3503.542509	1060260.500592	45.604647
3503.167997	1060208.658940	45.609652
3503.603597	1060135.979455	45.614657
3503.561219	1060089.378335	45.619661
3503.226731	1060032.809815	45.624666
3503.993232	1059970.185060	45.629671
3503.731972	1059918.418320	45.634676
3503.558193	1059866.540382	45.639681
3503.406232	1059807.435624	45.644685
3503.234731	1059749.489100	45.649690
3503.634303	1059690.195942	45.654695
3503.535290	1059643.407764	45.659700
3503.909172	1059576.605735	45.664705
3504.193760	1059511.358539	45.669709
3503.752869	1059453.164339	45.674714
3503.741471	1059382.185793	45.679719
3503.463396	1059328.104810	45.684724
3504.079246	1059251.435196	45.689729
3503.640644	1059191.407903	45.694733
3503.594663	1059133.915795	45.699738
3504.030138	1059069.601667	45.704743
3503.706944	1059012.924482	45.709748
3503.843813	1058947.502304	45.714753
3503.756747	1058892.422398	45.719757
3503.349397	1058830.170673	45.724762
3503.630002	1058765.396901	45.729767
3503.580147	1058713.776650	45.734772
3503.754161	1058655.183766	45.739777
3504.221942	1058599.142633	45.744781
3503.854581	1058530.908824	45.749786
3504.070670	1058462.192767	45.754791
3503.775405	1058401.458959	45.759796
3504.025551	1058328.882517	45.764801
3503.817282	1058256.669612	45.769805
3503.900122	1058190.380370	45.774810
3503.963625	1058113.496913	45.779815
3503.756696	1057991.186999	45.784820
3504.055758	1057799.042513	45.789825
3503.572201	1057548.155136	45.794829
3503.564331	1057257.001090	45.799834
3503.862137	1056880.701046	45.804839
3503.698246	1056455.788859	45.809844
3503.297345	1055959.665625	45.814849
3503.184235	1055401.574581	45.819853
3502.863948	1054775.795005	45.824858
3503.169259	1054095.470358	45.829863
3502.998422	1053359.990675	45.834868
3503.042815	1052522.065730	45.839873
3502.648266	1051628.533285	45.844877
3502.273967	1050664.435502	45.849882
3502.655167	1049633.377220	45.854887
3502.041443	1048528.178965	45.859892
3501.897506	1047347.493394	45.864897
3502.015776	1046093.237480	45.869901
3501.784935	1044751.266997	45.874906
3501.450514	1043338.671175	45.879911
3501.442822	1041853.489767	45.884916
3501.179842	1040276.432023	45.889921
3500.642349	1038610.806796	45.894925
3500.542611	1036872.760463	45.899930
3500.674123	1035066.516125	45.904935
3500.018748	1033173.790039	45.909940
3499.825153	1031195.450658	45.914945
3499.861360	1029118.082447	45.919949
3499.449619	1026976.271919	45.924954
3499.219850	1024755.596017	45.929959
3498.490725	1022437.556227	45.934964
3498.545888	1020024.537351	45.939969
3497.980513	1017552.942106	45.944973
3497.705681	1014988.371803	45.949978
3497.414577	1012340.270132	45.954983
3496.726246	1009615.677702	45.959988
3496.454752	1006795.393052	45.964993
3496.044590	1003913.898724	45.969997
3495.734433	1000930.285586	45.975002
3495.480626	997858.716591	45.980007
3494.601547	994727.029404	45.985012
3494.398224	991478.371387	45.990017
3493.958802	988162.833500	45.995021
3493.281130	984762.442000	46.000026
3492.881931	981287.999782	46.005031
3492.089229	977732.841831	46.010036
3491.960523	974072.593192	46.015041
3491.393455	970339.137917	46.020045
3490.515204	966539.856868	46.025050
3490.323236	962646.145098	46.030055
3489.337723	958659.139737	46.035060
3488.829394	954603.922548	46.040065
3488.126963	950566.030089	46.045069
3487.171951	946439.278897	46.050074
3487.051139	942230.876932	46.055079
3486.368336	937954.316150	46.060084
3485.730226	933576.141018	46.065089
3484.740973	929127.426640	46.070093
3483.676458	924589.904944	46.075098
3483.172492	919975.121817	46.080103
3482.482760	915291.229830	46.085108
3481.767299	910495.446930	46.090113
3480.797914	905637.454303	46.095117
3479.818458	900709.558747	46.100122
3479.024071	895677.850237	46.105127
3477.891435	890572.860364	46.110132
3476.990429	885387.957306	46.115137
3476.379881	880129.075692	46.120141
3475.345720	874769.118351	46.125146
3474.801468	869328.692430	46.130151
3473.439321	863818.058692	46.135156
3472.245756	858211.627942	46.140161
3471.329165	852540.538147	46.145165
3470.150051	846773.381125	46.150170
3469.626170	840935.270708	46.155175
3468.062513	835011.127329	46.160180
3467.455571	828992.099329	46.165185
3466.287759	822898.842045	46.170189
3465.304604	816710.247257	46.175194
3464.095120	810448.593742	46.180199
3462.763484	804102.413766	46.185204
3461.887858	797658.403576	46.190209
3460.749310	791153.699339	46.195213
3459.520966	784554.994532	46.200218
3458.330924	777882.484579	46.205223
3456.824944	771111.778275	46.210228
3455.714522	764262.613316	46.215233
3454.645405	757337.059133	46.220237
3453.417863	750324.867103	46.225242
3452.112725	743224.759838	46.230247
3450.943334	736043.011768	46.235252
3449.584089	728777.887703	46.240257
3448.214086	721417.996536	46.245261
3446.804687	713980.287102	46.250266
3445.827730	706450.592352	46.255271
3444.423111	698842.963087	46.260276
3442.616245	691161.405094	46.265281
3441.473744	683394.630247	46.270285
3439.657066	675543.827255	46.275290
3438.603772	667605.296257	46.280295
3436.921397	659599.365809	46.285300
3435.192315	651500.036383	46.290305
3433.605408	643325.056063	46.295309
3431.849460	635070.996444	46.300314
3430.674878	626751.530999	46.305319
3428.772329	618344.326461	46.310324
3427.108573	609864.589297	46.315329
3425.545341	601297.235696	46.320333
3423.549232	592674.990176	46.325338
3422.416830	583949.779343	46.330343
3420.172823	575153.436293	46.335348
3418.314149	566280.210747	46.340353
3416.417469	557335.795367	46.345357
3414.706261	548321.613778	46.350362
3412.980019	539233.418834	46.355367
3411.114311	530075.730745	46.360372
3409.042766	520827.771989	46.365377
3406.916836	511528.629957	46.370381
3404.844710	502153.374373	46.375386
3402.780813	492702.552289	46.380391
3400.874396	483186.864048	46.385396
3398.698769	473610.500010	46.390401
3396.755308	463949.082836	46.395405
3394.443859	454224.059788	46.400410
3392.440196	444439.013913	46.405415
3390.115575	434590.601836	46.410420
3387.620517	424667.712720	46.415425
3385.580281	414668.112110	46.420429
3383.134939	404627.083512	46.425434
3381.006252	394501.464127	46.430439
3378.403796	384336.473594	46.435444
3376.003105	374109.999933	46.440449
3373.112568	363823.639429	46.445453
3370.170860	353480.872905	46.450458
3367.946172	343084.909537	46.455463
3365.239109	332652.401261	46.460468
3362.190630	322154.714928	46.465473
3359.696418	311614.638440	46.470477
3356.778545	301025.166422	46.475482
3353.808156	290395.092863	46.480487
3351.069795	279722.208841	46.485492
3348.144041	268991.464366	46.490497
3345.120999	258232.912691	46.495501
3341.676611	247433.794932	46.500506
3338.811105	236584.782951	46.505511
3335.391726	225635.555654	46.510516
3332.272470	214715.968297	46.515521
3328.705430	203780.246424	46.520525
3324.773589	192816.956416	46.525530
3321.249845	181839.923275	46.530535
3317.520028	170848.474512	46.535540
3313.722562	159828.857515	46.540545
3309.318533	148810.566103	46.545549
3304.696483	137793.573674	46.550554
3300.730442	126765.754174	46.555559
3295.772553	115742.432193	46.560564
3291.195675	104723.558445	46.565569
3286.300056	93745.879745	46.570573
3280.525082	82767.932331	46.575578
3274.824195	71829.609262	46.580583
3268.197387	60956.857010	46.585588
3261.052349	50161.630887	46.590593
3252.198915	39456.191700	46.595597
3239.841891	28958.927219	46.600602
3198.121546	19414.957317	46.605607
3134.140967	10921.847027	46.610612
3066.494205	3334.644645	46.615617
2873.283729	395.485129	46.620621
2656.956523	390.503829	46.625626
2569.086382	388.624999	46.630631
2591.341484	388.974529	46.635636
2676.253218	367.555122	46.640641
2771.840534	345.642846	46.645645
2843.845489	341.423402	46.650650
2882.198446	337.408767	46.655655
2891.640383	345.596592	46.660660
2883.797269	348.344544	46.665665
2869.927533	335.746925	46.670669
2856.425925	325.847730	46.675674
2846.689105	325.306982	46.680679
2841.623786	332.699730	46.685684
2839.029459	332.503294	46.690689
2838.274499	334.260230	46.695693
2837.249307	337.574937	46.700698
2836.480730	321.492280	46.705703
2834.544152	325.199046	46.710708
2831.854153	322.670518	46.715713
2828.707554	321.621764	46.720717
2824.908986	319.020277	46.725722
2822.275003	323.720373	46.730727
2819.024771	313.021696	46.735732
2815.839285	306.591743	46.740737
2812.247692	306.071470	46.745741
2808.953149	301.721553	46.750746
2806.063383	303.363787	46.755751
2803.477417	312.006333	46.760756
2800.299909	300.534144	46.765761
2797.284828	293.862222	46.770765
2793.747521	310.642250	46.775770
2790.439231	296.596925	46.780775
2786.651319	293.930071	46.785780
2783.469255	294.329860	46.790785
2780.745656	294.446587	46.795789
2777.665819	303.241887	46.800794
2774.564598	297.926022	46.805799
2770.607099	298.491051	46.810804
2767.232152	300.179745	46.815809
2764.396587	293.853240	46.820813
2760.610099	288.510270	46.825818
2757.439594	296.557698	46.830823
2753.962367	291.423114	46.835828
2749.979310	289.644113	46.840833
2747.009699	288.148499	46.845837
2743.430581	298.429827	46.850842
2740.682835	285.355656	46.855847
2737.476914	289.463011	46.860852
2733.881794	292.773351	46.865857
2730.488377	285.289041	46.870861
2726.940244	293.230527	46.875866
2723.548018	292.079954	46.880871
2719.981570	287.071779	46.885876
2716.410865	283.745832	46.890881
2713.197623	286.414590	46.895885
2709.802972	286.873532	46.900890
2706.491356	279.903569	46.905895
2702.998739	288.454789	46.910900
2699.582211	283.878002	46.915905
2695.897114	290.732378	46.920909
2693.098475	281.331367	46.925914
2689.728557	282.984240	46.930919
2685.797246	282.703443	46.935924
2682.144339	281.424502	46.940929
2679.545916	284.371636	46.945933
2675.704160	273.320320	46.950938
2672.271091	274.913466	46.955943
2668.358856	276.936544	46.960948
2665.160907	274.691225	46.965953
2661.712658	260.961999	46.970957
2657.921408	271.102707	46.975962
2655.065271	270.986005	46.980967
2651.437609	273.389259	46.985972
2648.018673	262.177981	46.990977
2644.665892	277.999715	46.995981
2640.716896	279.155255	47.000986
2637.721404	260.237671	47.005991
2633.825746	256.058196	47.010996
2630.450306	264.091789	47.016001
2627.211726	262.897873	47.021005
2623.614811	271.987024	47.026010
2620.855679	251.045005	47.031015
2617.973802	257.681423	47.036020
2613.572344	258.520798	47.041025
2610.120483	258.247509	47.046029
2606.303813	261.503467	47.051034
2603.088457	255.582605	47.056039
2599.689259	258.190808	47.061044
2595.597115	252.796230	47.066049
2592.489475	254.789277	47.071053
2588.887654	268.977470	47.076058
2585.927250	252.135026	47.081063
2581.862997	249.522831	47.086068
2578.172452	251.936681	47.091073
2575.309201	244.219928	47.096077
2572.136462	252.841357	47.101082
2568.601713	265.465726	47.106087
2565.175129	258.450872	47.111092
2561.180426	259.443409	47.116097
2557.999264	250.295571	47.121101
2554.305940	253.161839	47.126106
2550.789187	245.424305	47.131111
2546.962683	251.841906	47.136116
2543.518092	247.571628	47.141121
2540.246704	245.879812	47.146125
2537.375402	246.283410	47.151130
2533.927197	246.535692	47.156135
2530.455079	247.287573	47.161140
2526.455132	237.230587	47.166145
2523.177028	244.780719	47.171149
2519.505207	248.756114	47.176154
2515.958141	234.510545	47.181159
2512.572436	246.913617	47.186164
2508.847253	242.735109	47.191169
2506.155634	250.495757	47.196173
2502.297166	237.491252	47.201178
2498.933443	242.728878	47.206183
2495.413284	236.439835	47.211188
2491.689034	232.491549	47.216193
2488.214407	230.841660	47.221197
2484.436789	255.295338	47.226202
2481.343898	243.284849	47.231207
2477.729022	233.111121	47.236212
2474.034009	247.788452	47.241217
2471.102198	228.997638	47.246221
2467.091881	240.197698	47.251226
2463.872683	244.562461	47.256231
2460.278570	238.196642	47.261236
2457.189990	225.359808	47.266241
2453.842844	232.539344	47.271245
2449.252699	237.715918	47.276250
2446.542132	236.007529	47.281255
2442.889983	224.171879	47.286260
2439.124163	228.791547	47.291265
2435.801664	226.979857	47.296269
2432.381301	232.244604	47.301274
2429.181293	225.359006	47.306279
2425.680531	233.369520	47.311284
2421.963505	227.604594	47.316289
2418.399408	228.489687	47.321293
2414.794448	227.151970	47.326298
2411.673963	226.276183	47.331303
2408.415924	236.564822	47.336308
2404.941518	225.311457	47.341313
2401.217632	222.377160	47.346317
2397.145524	232.319691	47.351322
2393.863826	216.463283	47.356327
2390.033041	219.906842	47.361332
2386.852540	215.576525	47.366337
2383.791217	212.346214	47.371341
2380.057129	240.567133	47.376346
2376.563737	221.616930	47.381351
2373.113145	211.052338	47.386356
2369.881158	225.393064	47.391361
2366.367035	215.382156	47.396365
2362.561679	218.396716	47.401370
2359.075416	228.415787	47.406375
2355.448195	229.562895	47.411380
2351.570357	221.097159	47.416385
2348.817316	222.702794	47.421389
2344.845800	228.515550	47.426394
2341.417251	229.647460	47.431399
2338.511664	217.737787	47.436404
2334.674089	217.949010	47.441409
2331.219813	217.125644	47.446413
2327.926856	216.832691	47.451418
2324.338907	215.739843	47.456423
2320.720680	213.584918	47.461428
2317.191973	216.618592	47.466433
2313.931126	224.075474	47.471437
2309.978372	220.385967	47.476442
2306.717032	221.248409	47.481447
2303.156779	214.833989	47.486452
2299.528401	214.022087	47.491457
2296.063651	219.441006	47.496461
2292.553990	223.381266	47.501466
2289.268773	213.601589	47.506471
2285.612610	209.717072	47.511476
2281.932279	213.742013	47.516481
2278.866969	218.408604	47.521485
2274.791946	230.697926	47.526490
2271.889348	211.046782	47.531495
2268.463574	205.859299	47.536500
2264.667837	223.846355	47.541505
2261.213832	209.424611	47.546509
2257.769925	222.537610	47.551514
2254.545454	210.999833	47.556519
2251.080739	219.240151	47.561524
2247.100966	212.684225	47.566529
2243.728374	212.990959	47.571533
2240.141721	220.544419	47.576538
2236.771422	207.207233	47.581543
2233.463688	210.851488	47.586548
2229.568228	210.648483	47.591553
2226.224698	206.891988	47.596557
2222.357076	213.374606	47.601562
2219.272705	213.597901	47.606567
2215.753225	212.092577	47.611572
2212.085602	212.856327	47.616577
2208.733358	212.175817	47.621581
2205.150563	217.405682	47.626586
2201.955212	209.001701	47.631591
2198.429517	215.950518	47.636596
2194.875141	212.646725	47.641601
2191.654028	214.170289	47.646605
2187.825812	214.053983	47.651610
2183.835776	210.602346	47.656615
2180.577230	211.442775	47.661620
2176.981079	213.211115	47.666625
2173.564917	205.557947	47.671629
2170.323825	203.443397	47.676634
2167.218111	205.267387	47.681639
2163.426754	203.496462	47.686644
2159.807696	216.525909	47.691649
2156.487547	196.627236	47.696653
2152.409207	211.007772	47.701658
2149.384676	210.122486	47.706663
2145.632500	204.097445	47.711668
2142.222516	206.718563	47.716673
2139.261010	198.842140	47.721677
2135.545523	204.875772	47.726682
2131.783338	195.792262	47.731687
2128.398620	197.722568	47.736692
2124.791202	199.400053	47.741697
2121.627317	200.648227	47.746701
2117.656154	204.755547	47.751706
2114.254638	198.272927	47.756711
2110.953241	207.000846	47.761716
2107.082513	200.729899	47.766721
2103.520404	199.282076	47.771725
2099.846047	212.049061	47.776730
2096.943865	209.039367	47.781735
2093.850921	197.973179	47.786740
2089.695287	202.266818	47.791745
2086.208326	195.422033	47.796749
2082.437495	203.335048	47.801754
2079.497705	191.611516	47.806759
2075.829992	199.191230	47.811764
2071.947957	196.887867	47.816769
2068.803271	201.293062	47.821773
2065.318060	207.833620	47.826778
2062.128110	193.463266	47.831783
2058.637236	195.027636	47.836788
2054.577506	209.431974	47.841793
2051.510972	205.949618	47.846797
2047.604889	203.336014	47.851802
2044.363228	197.439028	47.856807
2040.624464	200.897758	47.861812
2037.234963	196.495935	47.866817
2033.788130	186.367393	47.871821
2029.958191	206.300816	47.876826
2026.368805	190.619232	47.881831
2023.746372	184.033500	47.886836
2020.113374	202.155856	47.891841
2016.451169	185.944770	47.896845
2012.577632	192.852476	47.901850
2009.105747	189.567338	47.906855
2005.992217	200.110654	47.911860
2002.053807	197.691830	47.916865
1998.869313	187.496253	47.921869
1995.173512	192.797230	47.926874
1992.224461	194.738397	47.931879
1988.357769	193.252879	47.936884
1984.588956	204.102605	47.941889
1981.679544	186.002687	47.946893
1977.671645	192.103861	47.951898
1974.249107	196.264188	47.956903
1970.771784	188.770398	47.961908
1967.113553	185.110053	47.966913
1963.975044	198.966140	47.971917
1960.160893	194.690548	47.976922
1956.526022	184.157407	47.981927
1953.654091	195.515933	47.986932
1949.669920	194.482128	47.991937
1946.596615	178.191012	47.996941
1942.768920	182.696500	48.001946
1939.418273	183.972701	48.006951
1935.635307	186.562308	48.011956
1932.153037	187.381348	48.016961
1928.877410	193.730910	48.021965
1925.671836	193.085331	48.026970
1921.989462	178.920325	48.031975
1918.175424	179.238080	48.036980
1914.500346	201.893166	48.041985
1911.358521	182.777197	48.046989
1907.447665	197.425762	48.051994
1904.134579	191.656357	48.056999
1900.596513	194.420551	48.062004
1897.140086	188.185464	48.067009
1894.139588	179.498238	48.072013
1890.432671	187.601254	48.077018
1887.089639	186.127066	48.082023
1883.714246	185.630673	48.087028
1879.782173	188.056574	48.092033
1876.380066	187.850498	48.097037
1872.232391	184.637069	48.102042
1869.023183	185.393725	48.107047
1866.045754	190.526712	48.112052
1862.169672	206.116369	48.117057
1858.549845	188.273724	48.122061
1855.182677	192.381162	48.127066
1851.942286	181.169657	48.132071
1848.295857	187.927893	48.137076
1844.545151	186.603365	48.142081
1841.341128	188.551832	48.147085
1837.622880	192.815464	48.152090
1834.143870	192.292288	48.157095
1831.011353	186.532397	48.162100
1827.264689	179.404453	48.167105
1823.897780	186.782510	48.172109
1819.955943	188.773400	48.177114
1816.807120	179.136751	48.182119
1813.136258	186.207629	48.187124
1809.703437	191.901261	48.192129
1806.459880	185.691382	48.197133
1802.602111	184.451035	48.202138
1799.032462	194.732365	48.207143
1795.853316	184.652730	48.212148
1792.150815	191.417776	48.217153
1788.866958	192.473183	48.222157
1785.085642	190.759704	48.227162
1781.684441	181.785755	48.232167
1778.209330	183.972639	48.237172
1774.820454	175.595507	48.242177
1771.567299	185.503396	48.247181
1767.592710	195.670717	48.252186
1764.234637	180.041422	48.257191
1760.594041	172.555460	48.262196
1756.512318	189.322099	48.267201
1753.683730	186.284039	48.272205
1750.179848	184.968262	48.277210
1746.979478	188.901423	48.282215
1743.765611	180.028588	48.287220
1739.775408	177.454595	48.292225
1736.523158	183.707140	48.297229
1732.356923	184.024406	48.302234
1728.641198	179.661482	48.307239
1725.531538	184.591302	48.312244
1722.204256	177.271494	48.317249
1718.528146	172.699402	48.322253
1715.101990	182.249617	48.327258
1711.974820	185.992737	48.332263
1708.377543	178.426945	48.337268
1704.076744	185.873514	48.342273
1700.983975	175.869856	48.347277
1697.675448	187.633749	48.352282
1694.235598	177.075993	48.357287
1690.840594	177.827080	48.362292
1687.240462	178.465907	48.367297
1683.938210	176.922442	48.372301
1679.896831	180.635395	48.377306
1676.480606	186.207264	48.382311
1673.190835	167.807459	48.387316
1669.402698	184.240468	48.392321
1666.274874	183.118888	48.397325
1662.436309	177.298406	48.402330
1659.273413	178.345354	48.407335
1656.100864	176.432441	48.412340
1652.265510	184.647712	48.417345
1648.862189	172.155236	48.422349
1645.216227	187.093440	48.427354
1641.358210	176.325821	48.432359
1637.992685	163.929032	48.437364
1634.559277	171.512777	48.442369
1631.222621	171.932941	48.447373
1627.456369	178.583875	48.452378
1624.044195	180.973343	48.457383
1620.046428	174.517079	48.462388
1616.873622	173.058539	48.467393
1613.765981	175.910768	48.472397
1610.123057	168.935825	48.477402
1606.679689	173.166533	48.482407
1603.375766	185.034271	48.487412
1599.839165	182.175861	48.492417
1596.227551	168.409024	48.497421
1592.231370	184.286726	48.502426
1588.915093	174.357305	48.507431
1585.420050	170.451327	48.512436
1582.042388	175.331901	48.517441
1578.702987	174.512833	48.522445
1575.080743	165.089808	48.527450
1571.499004	186.779999	48.532455
1568.212838	177.887327	48.537460
1564.678256	174.899858	48.542465
1561.320144	166.949789	48.547469
1557.293068	182.797185	48.552474
1553.880668	169.739982	48.557479
1550.557271	174.926227	48.562484
1546.814994	183.413569	48.567489
1543.787179	167.227570	48.572493
1540.497539	175.808519	48.577498
1536.649691	177.388438	48.582503
1533.227899	166.006595	48.587508
1529.208254	167.948326	48.592513
1525.991265	169.602606	48.597517
1522.115479	166.896703	48.602522
1518.887912	162.113768	48.607527
1515.816327	166.198215	48.612532
1512.274358	178.446022	48.617537
1508.670039	174.183324	48.622541
1504.990749	181.022800	48.627546
1501.213952	173.385243	48.632551
1497.893471	172.386202	48.637556
1494.702972	176.056002	48.642561
1491.145516	176.845437	48.647565
1487.318269	170.637747	48.652570
1484.106769	172.353786	48.657575
1480.636066	172.184971	48.662580
1476.909228	174.048908	48.667585
1473.663212	165.514697	48.672589
1470.033493	175.351846	48.677594
1466.035751	178.343344	48.682599
1463.082539	167.791842	48.687604
1459.372444	171.629492	48.692609
1456.159918	159.653293	48.697613
1452.343484	173.562495	48.702618
1448.689085	171.355204	48.707623
1445.027480	168.612516	48.712628
1441.833041	166.565398	48.717633
1438.582932	162.529299	48.722637
1435.186799	168.666896	48.727642
1431.762652	177.299979	48.732647
1428.499159	167.586386	48.737652
1424.477888	162.858434	48.742657
1420.944767	160.531896	48.747661
1417.265107	163.759685	48.752666
1413.797068	168.223035	48.757671
1410.822767	161.872941	48.762676
1406.903649	164.018346	48.767681
1403.486717	161.441885	48.772685
1399.653633	174.542809	48.777690
1396.153993	158.880511	48.782695
1392.915613	152.737291	48.787700
1389.138463	165.052167	48.792705
1386.199351	160.700368	48.797709
1382.678137	161.123585	48.802714
1379.191906	159.919626	48.807719
1375.879238	160.907264	48.812724
1371.951246	171.928617	48.817729
1368.493147	157.373205	48.822733
1364.921828	172.091900	48.827738
1361.031471	168.778706	48.832743
1358.024658	168.949414	48.837748
1353.959735	170.317437	48.842753
1351.043120	156.186657	48.847757
1347.346886	167.111656	48.852762
1343.541692	170.404795	48.857767
1340.406029	166.347684	48.862772
1336.716390	173.891961	48.867777
1333.579657	167.368344	48.872781
1329.506574	166.270550	48.877786
1326.261983	161.247339	48.882791
1323.156374	163.409453	48.887796
1319.648627	166.150462	48.892801
1316.145806	163.785237	48.897805
1312.456917	169.255266	48.902810
1308.791742	176.834685	48.907815
1305.214628	166.572020	48.912820
1301.687886	180.425380	48.917825
1298.523129	170.022534	48.922829
1294.750143	166.900832	48.927834
1291.169916	176.110133	48.932839
1287.700100	168.217133	48.937844
1284.234660	169.496796	48.942849
1280.983564	158.740728	48.947853
1277.391166	175.856417	48.952858
1273.790279	159.489741	48.957863
1270.372446	151.597256	48.962868
1266.597031	172.856591	48.967873
1263.568590	164.633752	48.972877
1259.997940	163.572929	48.977882
1256.175671	164.944065	48.982887
1253.161753	169.598895	48.987892
1248.683378	163.336452	48.992897
1245.417394	163.881573	48.997901
1242.417514	162.109747	49.002906
1239.185993	161.963033	49.007911
1235.578898	159.951085	49.012916
1231.605463	163.201317	49.017921
1228.303303	156.570503	49.022925
1224.743725	165.713376	49.027930
1221.102590	161.631148	49.032935
1217.816343	153.798262	49.037940
1214.294966	172.821782	49.042945
1210.695439	161.388584	49.047949
1207.194542	151.684131	49.052954
1203.465547	169.401099	49.057959
1200.402144	159.919206	49.062964
1196.860462	163.628555	49.067969
1193.444122	164.551213	49.072973
1189.406916	165.170992	49.077978
1186.363627	166.618971	49.082983
1182.712083	147.866960	49.087988
1178.898760	169.722339	49.092993
1175.685231	146.787353	49.097997
1171.848154	166.802390	49.103002
1168.475800	169.711920	49.108007
1165.543785	157.101997	49.113012
1162.060889	151.877990	49.118017
1158.603013	158.811880	49.123021
1155.195852	151.036974	49.128026
1151.358186	155.308706	49.133031
1147.680943	162.180555	49.138036
1143.933427	162.688903	49.143041
1140.788131	145.853094	49.148045
1137.263058	155.469471	49.153050
1133.380924	161.736754	49.158055
1130.195763	159.811773	49.163060
1126.509069	162.839117	49.168065
1123.260922	155.340157	49.173069
1119.382344	158.127684	49.178074
1116.133139	162.242008	49.183079
1112.892647	149.222426	49.188084
1108.881345	165.230855	49.193089
1105.617961	155.326640	49.198093
1102.423991	150.851905	49.203098
1098.807948	162.555276	49.208103
1095.576247	141.841717	49.213108
1091.633627	161.906066	49.218113
1088.208407	165.578383	49.223117
1084.500102	161.889909	49.228122
1080.785147	149.172232	49.233127
1077.573126	154.548643	49.238132
1074.170462	153.485048	49.243137
1070.852946	145.582631	49.248141
1067.335717	148.380177	49.253146
1063.585029	147.567114	49.258151
1060.339995	161.456808	49.263156
1056.038958	161.514184	49.268161
1052.788615	150.365683	49.273165
1049.630093	151.513102	49.278170
1046.406887	154.985948	49.283175
1043.068822	147.486098	49.288180
1039.283469	154.543854	49.293185
1035.451710	146.649310	49.298189
1031.620699	162.751420	49.303194
1028.657011	157.170068	49.308199
1025.387458	152.331975	49.313204
1021.872807	152.262891	49.318209
1018.106769	150.112948	49.323213
1014.621781	141.334536	49.328218
1010.766053	157.057651	49.333223
1007.731661	150.607193	49.338228
1003.773995	149.301716	49.343233
1000.333690	141.737581	49.348237
997.050838	152.614886	49.353242
993.613497	154.662128	49.358247
990.139252	147.939109	49.363252
986.358576	152.753097	49.368257
983.195701	153.361721	49.373261
979.633380	150.509381	49.378266
976.030893	156.378666	49.383271
972.598872	151.466503	49.388276
968.898565	152.897469	49.393281
965.469346	144.912239	49.398285
961.831167	143.172439	49.403290
958.264001	146.463271	49.408295
955.401367	133.724435	49.413300
951.614233	148.559987	49.418305
948.278468	147.592550	49.423309
944.689360	139.218496	49.428314
941.092616	152.731523	49.433319
937.552391	146.450454	49.438324
934.108873	146.507690	49.443329
930.268420	145.750170	49.448333
926.710566	150.599019	49.453338
923.230686	154.082928	49.458343
920.085629	143.544277	49.463348
916.386121	144.705811	49.468353
913.368012	145.523093	49.473357
909.530195	147.802342	49.478362
905.675275	137.878236	49.483367
902.589371	140.060263	49.488372
898.702664	145.749902	49.493377
895.605591	135.474845	49.498381
892.253484	139.902316	49.503386
888.518162	155.800047	49.508391
885.365355	135.930633	49.513396
881.302625	151.032513	49.518401
878.070066	151.300988	49.523405
874.090036	143.528802	49.528410
870.838327	145.702311	49.533415
867.335206	145.903100	49.538420
863.401165	140.948609	49.543425
860.304222	139.289377	49.548429
857.191283	153.273731	49.553434
853.535617	166.386918	49.558439
850.452025	146.205581	49.563444
846.339215	146.198862	49.568449
842.833983	139.412387	49.573453
839.439412	144.159927	49.578458
836.173055	152.067425	49.583463
832.537110	135.154903	49.588468
828.858412	137.198968	49.593473
825.356701	146.164831	49.598477
821.828701	147.366659	49.603482
818.335072	146.384218	49.608487
814.858632	146.767383	49.613492
811.129682	138.465439	49.618497
807.715026	130.405691	49.623501
804.445586	144.275611	49.628506
800.896425	143.326422	49.633511
797.712644	136.158076	49.638516
793.835288	145.630918	49.643521
790.471086	137.750880	49.648525
786.816925	139.276036	49.653530
783.135892	146.466149	49.658535
780.071962	143.652075	49.663540
776.204587	141.640355	49.668545
772.833712	136.033746	49.673549
769.410275	147.706619	49.678554
765.563235	138.200394	49.683559
762.322901	136.449365	49.688564
758.954771	142.821069	49.693569
755.415998	138.923569	49.698573
752.078444	139.627050	49.703578
748.571668	140.115689	49.708583
744.904407	131.344169	49.713588
741.167485	147.004356	49.718593
737.674198	134.450295	49.723597
734.398335	143.165211	49.728602
730.628817	148.515253	49.733607
727.634616	131.012238	49.738612
724.328046	141.591671	49.743617
720.455266	140.482286	49.748621
717.007810	133.430734	49.753626
712.958984	148.907943	49.758631
709.612860	136.051191	49.763636
706.133632	146.646226	49.768641
702.847067	135.232827	49.773645
699.539332	130.790318	49.778650
695.532848	143.871615	49.783655
692.024756	140.846618	49.788660
688.625216	142.607488	49.793665
685.487155	141.154315	49.798669
682.024084	141.634587	49.803674
678.261233	134.255031	49.808679
674.943025	140.769172	49.813684
671.182762	138.846767	49.818689
667.654006	132.727739	49.823693
664.134727	130.812105	49.828698
660.857018	137.665642	49.833703
657.662579	142.799888	49.838708
653.728526	147.549799	49.843713
650.183842	143.314456	49.848717
646.840350	132.465232	49.853722
642.983825	147.510962	49.858727
639.403622	145.280334	49.863732
635.740705	152.006020	49.868737
632.521112	136.586976	49.873741
629.668873	129.382220	49.878746
625.658004	133.720517	49.883751
622.070694	133.170274	49.888756
618.838902	136.617497	49.893761
615.774830	148.320654	49.898765
611.784094	135.148686	49.903770
608.078079	140.197565	49.908775
604.567396	132.851977	49.913780
600.877054	128.500044	49.918785
597.668848	132.416330	49.923789
594.307711	131.382532	49.928794
590.486057	139.777644	49.933799
587.344121	131.468275	49.938804
583.706135	138.643970	49.943809
580.474309	116.594655	49.948813
576.637058	132.721724	49.953818
573.084486	144.577005	49.958823
569.923953	120.977595	49.963828
565.998960	127.344083	49.968833
562.777868	133.152634	49.973837
559.370723	130.040898	49.978842
555.544365	124.112173	49.983847
552.067405	120.516237	49.988852
548.445480	127.723130	49.993857
544.965568	128.654837	49.998861
541.609579	128.419022	50.003866
537.731833	135.200656	50.008871
534.388694	139.918432	50.013876
531.125780	137.503952	50.018881
527.688498	143.955943	50.023885
523.940839	144.263800	50.028890
520.450268	139.320037	50.033895
517.403584	131.943340	50.038900
513.681917	131.362571	50.043905
510.545698	119.381377	50.048909
507.097957	133.800653	50.053914
503.338741	134.495676	50.058919
499.699933	120.886642	50.063924
496.171501	135.573978	50.068929
492.647325	125.484548	50.073933
488.858071	126.480602	50.078938
484.970667	127.555321	50.083943
481.825152	136.056822	50.088948
478.591606	136.807680	50.093953
475.246668	129.144258	50.098957
472.077891	139.178356	50.103962
468.222678	139.651993	50.108967
464.589125	118.076959	50.113972
460.536667	133.489261	50.118977
457.279241	125.825405	50.123981
453.933804	121.464733	50.128986
450.432197	131.053046	50.133991
447.119311	140.076173	50.138996
443.248057	134.285454	50.144001
439.797855	134.261182	50.149005
436.633534	138.844299	50.154010
433.067979	137.360651	50.159015
429.655679	129.414000	50.164020
426.195580	143.995571	50.169025
422.507120	127.632859	50.174029
419.117601	128.108419	50.179034
415.501017	133.344765	50.184039
412.050242	124.452073	50.189044
408.470558	126.078287	50.194049
404.860039	134.798105	50.199053
401.752370	129.016035	50.204058
398.164175	138.572213	50.209063
394.883272	123.241109	50.214068
390.967830	120.486120	50.219073
387.160157	129.368244	50.224077
383.723601	130.711761	50.229082
380.196234	127.489565	50.234087
376.961923	127.629042	50.239092
373.336472	135.300773	50.244097
369.990527	127.443134	50.249101
366.644995	134.436744	50.254106
362.864436	138.289253	50.259111
359.733799	125.363696	50.264116
356.049184	129.839636	50.269121
352.266406	141.249928	50.274125
349.069710	134.684578	50.279130
345.577449	131.720008	50.284135
342.529863	128.136914	50.289140
338.253348	135.953317	50.294145
334.679716	131.047067	50.299149
331.564624	130.259547	50.304154
328.020235	140.992372	50.309159
323.954566	118.320871	50.314164
320.394735	121.297879	50.319169
317.445350	130.866147	50.324173
314.028982	125.342399	50.329178
310.663752	134.200893	50.334183
307.307365	137.604423	50.339188
303.206729	133.108155	50.344193
299.958481	123.245649	50.349197
296.445294	120.031520	50.354202
293.212117	122.434964	50.359207
289.918743	131.595511	50.364212
285.809382	125.254682	50.369217
281.992512	127.568999	50.374221
278.870306	122.993770	50.379226
275.111752	131.645667	50.384231
271.725955	127.827063	50.389236
267.926206	133.011270	50.394241
264.895424	117.737688	50.399245
261.500996	127.782111	50.404250
257.990785	133.418465	50.409255
254.722161	123.227383	50.414260
250.937513	131.233669	50.419265
247.343575	129.108338	50.424269
243.546144	128.714961	50.429274
240.096866	126.619203	50.434279
237.222631	124.289927	50.439284
233.443929	145.157871	50.444289
230.151180	132.054960	50.449293
226.619695	128.157655	50.454298
222.635492	137.591604	50.459303
219.111924	129.775439	50.464308
215.794111	129.137489	50.469313
212.148583	122.751053	50.474317
208.758915	124.279288	50.479322
204.715470	130.479384	50.484327
201.854844	125.071743	50.489332
198.306488	125.376454	50.494337
194.977139	130.664993	50.499341
191.553175	124.501815	50.504346
187.920579	132.588275	50.509351
184.357246	130.098822	50.514356
180.811480	125.267875	50.519361
177.358674	120.511446	50.524365
173.891449	126.666563	50.529370
170.027291	129.515176	50.534375
166.716793	119.554719	50.539380
163.398110	140.653979	50.544385
159.657220	131.808591	50.549389
156.411967	127.773172	50.554394
152.677580	141.944881	50.559399
149.191286	132.313678	50.564404
145.705526	138.139510	50.569409
141.987920	126.917956	50.574413
139.088031	124.838811	50.579418
135.048555	133.755223	50.584423
131.893145	121.639022	50.589428
128.199737	132.919616	50.594433
124.667089	123.414875	50.599437
121.243117	122.119132	50.604442
117.495778	136.603061	50.609447
114.598661	127.114060	50.614452
110.912228	136.389948	50.619457
107.300776	128.467329	50.624461
103.172029	128.391106	50.629466
99.764077	126.507216	50.634471
96.707417	123.298563	50.639476
92.868217	122.484120	50.644481
89.767899	132.035384	50.649485
85.991642	131.564218	50.654490
82.520615	135.571722	50.659495
79.516451	134.053320	50.664500
76.099134	133.322973	50.669505
72.453731	124.547009	50.674509
68.705537	129.952569	50.679514
65.281214	139.206674	50.684519
61.935501	125.560960	50.689524
58.094589	127.726761	50.694529
54.641274	134.698960	50.699533
51.058756	125.839121	50.704538
47.327746	121.269917	50.709543
43.958420	119.955421	50.714548
40.495611	127.036725	50.719553
37.222321	121.114517	50.724557
34.110959	121.271536	50.729562
30.288720	124.554087	50.734567
26.839316	121.818011	50.739572
22.886543	129.685473	50.744577
19.195528	134.517114	50.749581
16.091649	115.683615	50.754586
12.693018	133.969594	50.759591
9.055024	128.818865	50.764596
5.573800	125.713964	50.769601
2.166577	127.604111	50.774605