Thu Jun 16 11:44:10 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
-0.101376	75.210617	0.000000
0.003662	82.676588	0.005005
0.013013	95.376062	0.010010
0.081033	70.988507	0.015014
-0.245382	77.408130	0.020019
-0.194550	76.344208	0.025024
-0.513277	68.718064	0.030029
-1.125534	69.968228	0.035034
-0.835740	65.479528	0.040038
-1.149498	53.204222	0.045043
-1.392255	36.161814	0.050048
-1.637856	39.100309	0.055053
-2.007326	39.127597	0.060058
-2.103926	17.290979	0.065062
-2.540234	19.777979	0.070067
-3.114096	14.189973	0.075072
-3.699185	14.263153	0.080077
-4.306957	21.846296	0.085082
-3.918435	21.894331	0.090086
-4.438741	16.391885	0.095091
-4.262839	16.094748	0.100096
-4.489946	15.639872	0.105101
-5.070550	13.242730	0.110106
-5.449586	10.988177	0.115110
-5.964769	14.997602	0.120115
-5.653445	11.930896	0.125120
-5.865864	13.208308	0.130125
-6.129371	18.503915	0.135130
-5.826731	10.367582	0.140134
-6.636768	12.804272	0.145139
-6.875255	15.206690	0.150144
-6.788591	14.851100	0.155149
-7.138998	16.230730	0.160154
-7.985774	12.465849	0.165158
-8.511172	13.098591	0.170163
-8.315157	7.742855	0.175168
-8.409103	23.302320	0.180173
-8.688712	15.106824	0.185178
-8.594694	20.075112	0.190182
-8.991545	30.114887	0.195187
-9.369639	12.056548	0.200192
-9.885541	13.656493	0.205197
-10.330454	29.051598	0.210202
-10.456479	13.753746	0.215206
-10.438832	20.756646	0.220211
-10.590449	13.057831	0.225216
-10.490810	12.865735	0.230221
-11.684924	12.420610	0.235226
-12.039807	3.969718	0.240230
-12.215127	17.957370	0.245235
-12.141799	7.266924	0.250240
-12.056419	3.735611	0.255245
-12.230826	10.424170	0.260250
-12.205790	23.018786	0.265254
-12.723806	17.282648	0.270259
-13.267069	6.794624	0.275264
-13.342553	17.886789	0.280269
-13.458069	19.606135	0.285274
-13.802632	13.431629	0.290278
-14.647420	18.055676	0.295283
-14.907055	12.389109	0.300288
-15.102511	6.207821	0.305293
-15.466973	18.677977	0.310298
-15.268747	16.035819	0.315302
-15.548128	14.387100	0.320307
-15.736250	18.998522	0.325312
-15.437160	15.896742	0.330317
-16.046702	22.867839	0.335322
-16.074125	9.105116	0.340326
-16.681105	13.795718	0.345331
-16.660706	18.706226	0.350336
-17.410537	10.897520	0.355341
-18.087323	10.727581	0.360346
-18.103574	9.135809	0.365350
-18.574132	10.500274	0.370355
-18.324947	14.737055	0.375360
-18.676751	17.310224	0.380365
-18.743376	4.431503	0.385370
-18.101607	15.616351	0.390374
-18.580856	22.475156	0.395379
-19.457705	6.167175	0.400384
-19.172536	10.398107	0.405389
-19.807893	8.539980	0.410394
-20.620063	8.552626	0.415398
-21.397381	12.681235	0.420403
-21.087414	16.105627	0.425408
-21.327241	9.218114	0.430413
-21.483150	20.348234	0.435418
-21.501946	13.980595	0.440422
-21.621122	15.498110	0.445427
-21.619073	20.072382	0.450432
-21.740316	16.728125	0.455437
-22.520817	14.336198	0.460442
-22.884102	23.926877	0.465446
-23.260024	16.215803	0.470451
-23.530957	11.539213	0.475456
-22.997523	17.857262	0.480461
-23.515803	18.805702	0.485466
-24.499657	4.636448	0.490470
-25.164122	16.535455	0.495475
-24.520465	14.591548	0.500480
-24.487431	17.143146	0.505485
-24.920452	15.536590	0.510490
-25.152561	20.144626	0.515494
-25.300683	17.882693	0.520499
-25.679588	13.259559	0.525504
-25.954566	12.321106	0.530509
-26.633509	19.467336	0.535514
-26.821094	14.971021	0.540518
-26.752093	22.017820	0.545523
-27.279110	23.432557	0.550528
-26.806865	24.763253	0.555533
-27.026017	9.262972	0.560538
-27.885127	3.554304	0.565542
-28.008769	16.640998	0.570547
-27.942193	9.136879	0.575552
-28.232309	9.397588	0.580557
-28.987606	21.939438	0.585562
-29.295557	21.409530	0.590566
-29.380178	16.940199	0.595571
-29.552442	17.690581	0.600576
-29.832564	16.241462	0.605581
-29.897343	19.117319	0.610586
-29.843840	9.357488	0.615590
-30.725330	21.913187	0.620595
-30.907399	19.617304	0.625600
-31.288006	16.632782	0.630605
-31.400323	13.523225	0.635610
-31.423362	16.144071	0.640614
-31.376171	22.022180	0.645619
-31.598202	13.771694	0.650624
-32.001539	22.529750	0.655629
-32.508692	14.014836	0.660634
-32.444624	0.395934	0.665638
-33.770143	18.798573	0.670643
-33.998018	24.523649	0.675648
-33.372894	12.881956	0.680653
-33.726197	18.414470	0.685658
-33.852817	15.556672	0.690662
-34.269750	8.473006	0.695667
-34.268362	22.042469	0.700672
-34.443485	11.785522	0.705677
-35.091420	22.197666	0.710682
-35.381846	15.913687	0.715686
-36.095170	19.579104	0.720691
-36.227306	17.407559	0.725696
-35.940976	21.914332	0.730701
-36.159466	25.573247	0.735706
-35.997899	10.018929	0.740710
-37.121362	22.213592	0.745715
-37.448025	12.331216	0.750720
-37.424392	15.214461	0.755725
-37.282087	12.857082	0.760730
-37.436839	20.337638	0.765734
-38.067573	32.199710	0.770739
-38.686097	14.695091	0.775744
-38.727642	27.133493	0.780749
-39.085652	14.556656	0.785754
-39.103910	5.457922	0.790758
-39.148591	19.770157	0.795763
-39.150391	12.272897	0.800768
-39.393074	13.908785	0.805773
-40.586907	22.457025	0.810778
-40.637925	15.039322	0.815782
-41.038300	22.218243	0.820787
-41.002058	16.227045	0.825792
-40.990834	19.688475	0.830797
-41.069566	21.332883	0.835802
-40.784668	10.092702	0.840806
-41.787858	24.893140	0.845811
-42.117217	13.035288	0.850816
-42.404132	19.032832	0.855821
-42.764629	23.343535	0.860826
-42.446275	3.290879	0.865830
-42.634432	18.230776	0.870835
-43.387611	19.026058	0.875840
-43.696392	-0.987768	0.880845
-44.245335	8.152057	0.885850
-43.837196	10.950449	0.890854
-44.052872	20.270493	0.895859
-44.530383	16.134330	0.900864
-44.719168	13.485295	0.905869
-45.480345	17.143132	0.910874
-45.262070	19.236851	0.915878
-45.663759	13.077215	0.920883
-45.945210	21.355898	0.925888
-46.049666	14.023384	0.930893
-46.098984	12.346020	0.935898
-46.805780	18.655738	0.940902
-47.051153	18.629768	0.945907
-47.185432	14.604987	0.950912
-47.490956	13.645145	0.955917
-47.934425	17.726576	0.960922
-47.542255	9.218918	0.965926
-47.818434	20.383906	0.970931
-48.036740	10.360310	0.975936
-48.567201	11.019442	0.980941
-49.044465	15.158645	0.985946
-48.943079	14.363391	0.990950
-48.932535	9.263136	0.995955
-49.632975	3.403060	1.000960
-50.291420	16.400164	1.005965
-50.523163	21.624129	1.010970
-50.533094	5.986779	1.015974
-50.772148	19.731620	1.020979
-50.847736	24.291298	1.025984
-50.871464	18.368413	1.030989
-50.955833	13.854353	1.035994
-51.454913	9.498899	1.040998
-52.305877	18.170221	1.046003
-52.361791	9.545227	1.051008
-52.237187	26.317024	1.056013
-52.128647	21.072223	1.061018
-52.244264	16.270524	1.066022
-53.154093	13.436109	1.071027
-53.449305	12.852798	1.076032
-53.527711	11.772060	1.081037
-53.899190	14.856248	1.086042
-53.810104	8.396796	1.091046
-54.474582	18.730381	1.096051
-55.147276	13.383349	1.101056
-55.287527	12.982587	1.106061
-55.626723	12.232620	1.111066
-55.467641	8.409051	1.116070
-55.744006	18.595924	1.121075
-55.892231	11.097116	1.126080
-55.479810	17.273466	1.131085
-55.800786	29.837956	1.136090
-56.446247	10.730049	1.141094
-56.984687	14.247194	1.146099
-56.990221	19.761599	1.151104
-57.068229	18.720158	1.156109
-57.473865	20.821785	1.161114
-57.826145	20.723215	1.166118
-58.392603	15.550210	1.171123
-58.741890	17.951210	1.176128
-58.407824	18.484537	1.181133
-58.813276	10.400609	1.186138
-58.702021	8.709337	1.191142
-59.725854	19.462393	1.196147
-59.988711	15.587802	1.201152
-60.009100	19.313024	1.206157
-60.524911	22.126785	1.211162
-59.945932	12.485411	1.216166
-60.466731	17.102285	1.221171
-60.360922	16.307583	1.226176
-60.714254	15.893596	1.231181
-61.515712	17.395519	1.236186
-61.488100	9.450252	1.241190
-61.790263	20.698752	1.246195
-62.042526	9.406962	1.251200
-62.657951	10.998990	1.256205
-62.972301	25.371577	1.261210
-63.096003	21.963109	1.266214
-63.541032	22.396711	1.271219
-63.469676	6.989404	1.276224
-63.031933	22.403182	1.281229
-63.536113	16.558219	1.286234
-63.731541	12.820169	1.291238
-64.550871	20.964490	1.296243
-64.797475	11.014136	1.301248
-64.923847	7.816539	1.306253
-65.510576	17.411781	1.311258
-65.011291	7.978814	1.316262
-65.357173	10.356067	1.321267
-65.841296	10.254525	1.326272
-66.353066	7.612898	1.331277
-66.804300	15.542386	1.336282
-66.666807	17.243103	1.341286
-66.820393	17.240636	1.346291
-66.889443	22.133468	1.351296
-67.322796	6.490134	1.356301
-68.400626	18.261728	1.361306
-68.222369	9.022691	1.366310
-68.241552	18.593591	1.371315
-68.210620	11.690439	1.376320
-68.124158	14.309563	1.381325
-68.377485	13.275787	1.386330
-68.938481	3.397719	1.391334
-69.673390	16.325971	1.396339
-69.791536	16.654153	1.401344
-69.673725	11.411277	1.406349
-69.938049	12.019917	1.411354
-70.116612	14.384317	1.416358
-70.739031	8.076782	1.421363
-71.072146	14.144012	1.426368
-71.198373	24.160266	1.431373
-71.576257	22.940889	1.436378
-71.207334	5.782841	1.441382
-71.551790	13.371495	1.446387
-72.707779	18.944522	1.451392
-73.037603	8.202818	1.456397
-73.496591	12.244787	1.461402
-72.667765	19.386301	1.466406
-72.991028	9.573513	1.471411
-73.139668	1.127811	1.476416
-73.194386	13.716748	1.481421
-73.364096	21.852068	1.486426
-74.000469	7.298170	1.491430
-74.758131	17.335115	1.496435
-75.277822	7.875216	1.501440
-75.301289	10.834510	1.506445
-75.340558	14.719709	1.511450
-74.924414	17.101150	1.516454
-75.093809	12.296898	1.521459
-75.611992	10.144171	1.526464
-76.004930	13.210596	1.531469
-76.372368	8.326610	1.536474
-76.514029	6.892496	1.541478
-77.494626	9.195392	1.546483
-77.821680	14.089524	1.551488
-77.241308	15.672358	1.556493
-77.605183	19.140235	1.561498
-78.116096	3.426757	1.566502
-78.056706	12.534810	1.571507
-78.083882	15.999130	1.576512
-78.477294	2.851337	1.581517
-79.018058	25.978607	1.586522
-79.418957	20.342196	1.591526
-80.066976	11.641724	1.596531
-80.072097	20.685072	1.601536
-80.097441	10.186639	1.606541
-80.188160	16.274678	1.611546
-79.891185	6.137322	1.616550
-80.029549	8.023221	1.621555
-81.168951	17.956433	1.626560
-81.490602	14.993938	1.631565
-81.405564	13.049317	1.636570
-81.681367	15.735809	1.641574
-81.992587	18.705566	1.646579
-82.363675	8.825017	1.651584
-81.640863	14.793307	1.656589
-82.690786	11.907468	1.661594
-83.059074	11.849921	1.666598
-83.386673	23.340477	1.671603
-83.431350	16.883990	1.676608
-82.981722	15.169154	1.681613
-84.046878	23.868776	1.686618
-84.044643	14.735185	1.691622
-84.739822	26.695013	1.696627
-84.969288	15.436845	1.701632
-84.601886	20.996555	1.706637
-84.921810	9.674024	1.711642
-85.292238	13.187080	1.716646
-85.764796	14.827023	1.721651
-86.254678	14.269967	1.726656
-86.455976	23.940911	1.731661
-86.623210	18.116820	1.736666
-86.465984	8.752617	1.741670
-86.730090	18.339033	1.746675
-86.798459	23.169995	1.751680
-87.600038	12.257551	1.756685
-88.121585	14.940460	1.761690
-88.076063	6.700816	1.766694
-87.970308	19.706286	1.771699
-88.342324	25.315391	1.776704
-87.866505	17.138007	1.781709
-89.057938	19.688841	1.786714
-89.253615	26.279700	1.791718
-89.732091	14.210128	1.796723
-89.757526	17.277181	1.801728
-89.898467	22.119347	1.806733
-89.989487	22.279283	1.811738
-90.654659	21.412126	1.816742
-91.338380	24.363143	1.821747
-91.405846	12.167737	1.826752
-91.350270	15.862349	1.831757
-91.644437	27.858306	1.836762
-91.410555	12.927564	1.841766
-91.449140	20.576853	1.846771
-91.564161	25.142947	1.851776
-92.152745	17.550192	1.856781
-92.954110	26.807116	1.861786
-92.956538	22.501187	1.866790
-92.885054	19.030473	1.871795
-93.525652	16.424246	1.876800
-93.718833	13.489354	1.881805
-94.707487	11.849441	1.886810
-94.831159	14.504181	1.891814
-94.669476	24.262424	1.896819
-94.668404	23.283976	1.901824
-94.629545	14.271497	1.906829
-94.856691	24.127543	1.911834
-95.057615	19.184171	1.916838
-95.637297	17.617545	1.921843
-95.803934	17.615263	1.926848
-96.163999	22.401008	1.931853
-96.572454	19.965756	1.936858
-96.398218	17.734900	1.941862
-96.655101	20.554308	1.946867
-97.488825	17.190085	1.951872
-97.627136	13.581994	1.956877
-98.225049	23.033278	1.961882
-97.995273	12.072717	1.966886
-97.825555	7.736764	1.971891
-97.922292	16.244864	1.976896
-98.695646	18.258792	1.981901
-99.162811	14.979995	1.986906
-99.099816	9.346735	1.991910
-99.407826	16.130080	1.996915
-99.452581	11.168199	2.006912
-99.619032	16.328812	2.016909
-99.435830	9.164988	2.026906
-98.595909	16.601992	2.036902
-97.963842	16.085862	2.046899
-97.249751	11.298346	2.056896
-97.204490	13.451456	2.066893
-96.470497	19.475843	2.076890
-95.587381	18.451589	2.086886
-95.570031	15.533985	2.096883
-94.874345	17.526212	2.106880
-93.959228	21.151100	2.116877
-93.591111	16.399375	2.126874
-93.713434	23.495687	2.136870
-93.587425	9.871517	2.146867
-92.308795	21.808166	2.156864
-91.845886	19.688109	2.166861
-90.939316	19.006152	2.176858
-90.789036	21.414983	2.186854
-90.720743	5.956047	2.196851
-90.300140	16.737624	2.206848
-89.280023	16.523537	2.216845
-89.035808	19.981042	2.226842
-88.012708	17.178643	2.236838
-87.507225	14.895628	2.246835
-86.999425	14.866471	2.256832
-87.470318	9.238353	2.266829
-86.764749	22.549199	2.276826
-86.101113	26.112130	2.286822
-85.210858	10.192660	2.296819
-84.592436	13.783557	2.306816
-84.527231	11.966545	2.316813
-84.014930	16.332075	2.326810
-83.266917	14.642647	2.336806
-82.866801	12.968635	2.346803
-82.493459	11.538044	2.356800
-81.805559	12.927129	2.366797
-81.416939	20.994603	2.376794
-80.872130	17.404758	2.386790
-79.826814	13.339994	2.396787
-79.774457	7.951323	2.406784
-79.610012	18.676408	2.416781
-79.077881	18.302838	2.426778
-78.740725	17.944056	2.436774
-77.924583	13.558598	2.446771
-77.079294	9.183684	2.456768
-76.927615	12.372047	2.466765
-76.437283	14.853882	2.476762
-75.500773	13.739758	2.486758
-75.103393	9.517398	2.496755
-74.922386	9.879383	2.506752
-74.829330	10.358535	2.516749
-73.748110	9.239610	2.526746
-73.560159	14.124834	2.536742
-72.553448	14.530682	2.546739
-71.957338	17.430900	2.556736
-72.010743	14.500739	2.566733
-71.648240	14.804627	2.576730
-70.674146	24.639559	2.586726
-70.167172	11.214142	2.596723
-70.085943	26.735682	2.606720
-69.333123	8.573174	2.616717
-69.101126	16.824875	2.626714
-68.028313	16.657351	2.636710
-67.647736	9.113943	2.646707
-67.503707	16.544263	2.656704
-67.047898	8.000236	2.666701
-66.320156	14.732276	2.676698
-65.688895	17.537835	2.686694
-65.467868	9.130794	2.696691
-64.263951	11.680702	2.706688
-64.027460	15.375221	2.716685
-63.943428	12.250816	2.726682
-63.944368	10.482469	2.736678
-62.977021	10.121234	2.746675
-62.476657	6.586053	2.756672
-61.432655	17.645850	2.766669
-61.034328	15.718617	2.776666
-60.833777	13.378970	2.786662
-60.552966	15.064402	2.796659
-59.938109	10.748859	2.806656
-59.634105	14.105409	2.816653
-58.854659	16.325412	2.826650
-58.064057	22.454443	2.836646
-58.027666	12.615584	2.846643
-57.069273	9.869668	2.856640
-56.740522	21.510355	2.866637
-56.441173	7.761424	2.876634
-55.851317	10.620152	2.886630
-55.127667	19.304455	2.896627
-54.603501	11.108538	2.906624
-54.646422	14.210526	2.916621
-53.843620	10.366709	2.926618
-53.021069	9.254383	2.936614
-52.955755	2.969124	2.946611
-52.198870	7.889726	2.956608
-51.831060	6.620518	2.966605
-51.512053	7.753290	2.976602
-50.277124	14.361758	2.986598
-50.032532	16.853437	2.996595
-49.817888	16.547648	3.006592
-49.621848	9.217330	3.016589
-48.552748	15.020445	3.026586
-48.022155	10.081009	3.036582
-47.866977	5.607673	3.046579
-47.537038	7.153808	3.056576
-46.814547	8.043876	3.066573
-46.397567	7.197171	3.076570
-45.625114	19.944302	3.086566
-45.004243	8.359288	3.096563
-45.033898	4.481317	3.106560
-44.415481	13.103888	3.116557
-43.812652	8.853305	3.126554
-43.496506	13.064414	3.136550
-42.698618	10.502677	3.146547
-41.938084	6.441569	3.156544
-41.740328	12.051350	3.166541
-41.500812	16.651276	3.176538
-40.314218	17.534930	3.186534
-39.974810	17.082283	3.196531
-40.135659	8.865329	3.206528
-39.664444	17.103876	3.216525
-38.846758	11.142192	3.226522
-38.186708	17.061459	3.236518
-37.350225	17.683866	3.246515
-36.991671	16.079893	3.256512
-37.124548	12.856252	3.266509
-36.430587	21.026431	3.276506
-35.556471	15.864078	3.286502
-35.260690	8.856386	3.296499
-35.203944	10.280189	3.306496
-34.335525	13.597944	3.316493
-33.702702	7.335211	3.326490
-32.805286	19.392415	3.336486
-32.816130	15.181063	3.346483
-32.552537	15.814035	3.356480
-31.668648	7.078209	3.366477
-30.972031	14.778745	3.376474
-30.842807	14.916516	3.386470
-30.548429	14.209694	3.396467
-29.466849	18.252973	3.406464
-29.113250	16.178889	3.416461
-28.883022	15.670497	3.426458
-28.059414	18.262717	3.436454
-27.695598	14.798256	3.446451
-27.390082	14.670712	3.456448
-26.207535	11.752330	3.466445
-26.151774	14.192588	3.476442
-25.981366	8.762179	3.486438
-25.507868	20.964020	3.496435
-24.888345	13.451651	3.506432
-24.322562	12.292464	3.516429
-23.180797	12.448661	3.526426
-23.184479	4.748527	3.536422
-22.549179	9.841693	3.546419
-22.236807	11.345641	3.556416
-22.209476	11.722849	3.566413
-21.284247	9.265668	3.576410
-20.642463	18.471331	3.586406
-19.471949	14.645477	3.596403
-19.936080	13.694371	3.606400
-19.233860	13.138997	3.616397
-18.833362	11.914222	3.626394
-18.374339	21.745334	3.636390
-17.708632	18.093334	3.646387
-17.009287	18.066904	3.656384
-16.276455	13.250959	3.666381
-16.162032	11.978681	3.676378
-15.806685	10.819944	3.686374
-15.809460	15.032148	3.696371
-14.821588	8.800333	3.706368
-13.912129	13.647229	3.716365
-13.398095	8.346135	3.726362
-13.527649	11.265623	3.736358
-12.860064	21.765875	3.746355
-11.620926	17.139779	3.756352
-11.524574	11.876691	3.766349
-11.218592	15.088948	3.776346
-11.183955	15.444798	3.786342
-10.034982	11.697628	3.796339
-9.482994	14.223956	3.806336
-9.561403	20.170038	3.816333
-9.112850	15.807399	3.826330
-7.943202	15.014019	3.836326
-7.537645	24.255120	3.846323
-6.582473	17.531401	3.856320
-6.456813	15.412999	3.866317
-6.408144	17.723498	3.876314
-6.139983	6.854344	3.886310
-5.311068	20.462747	3.896307
-4.770653	5.485463	3.906304
-3.472709	19.753942	3.916301
-3.797822	14.783446	3.926298
-3.782856	15.649779	3.936294
-3.143064	23.972543	3.946291
-2.487428	35.028242	3.956288
-1.778808	59.146993	3.966285
-1.557092	60.062730	3.976282
-1.191127	77.762637	3.986278
-0.810482	99.958477	3.996275
-0.294182	109.053360	4.006272
0.000000	144.418492	4.011277
0.214556	140.244677	4.016282
0.295541	156.812123	4.021286
0.545342	156.320558	4.026291
0.709424	164.506259	4.031296
0.765612	158.205683	4.036301
1.195558	175.933466	4.041306
0.953699	185.348504	4.046310
1.174661	190.179459	4.051315
1.090909	200.678929	4.056320
0.963625	197.508964	4.061325
1.362862	182.139728	4.066330
1.468194	192.998715	4.071334
1.291005	179.418531	4.076339
0.849298	168.807262	4.081344
1.175168	184.652276	4.086349
1.203584	185.573717	4.091354
1.192159	200.811530	4.096358
1.194464	195.246333	4.101363
1.435026	200.759698	4.106368
1.153430	203.385815	4.111373
1.311440	198.547322	4.116378
0.946529	198.693919	4.121382
1.181588	193.356527	4.126387
1.145799	195.621988	4.131392
1.249023	187.449655	4.136397
1.613213	201.998353	4.141402
1.273953	201.493736	4.146406
1.375811	190.913773	4.151411
1.106224	185.578191	4.156416
1.182134	199.602628	4.161421
1.568135	197.413406	4.166426
1.133117	203.208690	4.171430
0.962571	189.957792	4.176435
1.297681	200.277749	4.181440
1.432804	195.099031	4.186445
1.526034	194.235565	4.191450
1.313805	200.807732	4.196454
1.583685	202.833365	4.201459
1.667247	190.394327	4.206464
1.495082	195.743958	4.211469
1.524431	198.130162	4.216474
1.672025	206.355309	4.221478
1.643952	203.165791	4.226483
1.665460	196.645999	4.231488
1.307611	203.201388	4.236493
1.542512	204.660310	4.241498
1.172573	206.827486	4.246502
1.521710	204.849556	4.251507
1.592910	201.547939	4.256512
1.268171	204.465112	4.261517
1.518314	196.100290	4.266522
1.791341	205.830002	4.271526
2.024577	187.427445	4.276531
1.700411	206.104827	4.281536
1.399671	201.919862	4.286541
1.823745	208.081053	4.291546
1.492960	202.570502	4.296550
1.579531	205.239268	4.301555
1.531294	216.132133	4.306560
1.691596	229.406098	4.311565
2.125283	221.964327	4.316570
1.901724	221.717710	4.321574
1.706972	205.326980	4.326579
1.960365	204.511531	4.331584
1.656209	198.146576	4.336589
1.860720	194.484941	4.341594
1.610327	199.240383	4.346598
1.638097	212.494010	4.351603
1.859994	214.789402	4.356608
1.601355	227.561289	4.361613
1.734950	223.899626	4.366618
1.849252	228.043925	4.371622
2.059150	225.655119	4.376627
2.018012	231.386903	4.381632
1.751098	225.677951	4.386637
1.787459	228.791760	4.391642
1.608502	234.839817	4.396646
2.046037	226.681966	4.401651
2.003805	233.113490	4.406656
2.041517	228.265172	4.411661
2.071635	233.324098	4.416666
2.115206	240.385264	4.421670
2.182917	226.859572	4.426675
2.062485	239.209869	4.431680
1.890319	226.491645	4.436685
1.949314	231.129872	4.441690
1.926636	237.993528	4.446694
2.186136	232.723213	4.451699
2.218467	229.631438	4.456704
1.632149	237.136755	4.461709
2.198950	237.628774	4.466714
1.659807	241.611140	4.471718
1.735772	247.718689	4.476723
1.677792	246.990307	4.481728
2.049006	255.855001	4.486733
2.296903	258.090659	4.491738
2.298524	254.361812	4.496742
2.239394	260.812910	4.501747
2.528460	270.226587	4.506752
2.314851	256.023628	4.511757
2.207822	266.612523	4.516762
2.198577	270.392890	4.521766
2.327995	269.061933	4.526771
2.337290	263.139117	4.531776
2.428837	274.899381	4.536781
2.705128	269.771598	4.541786
2.413729	263.423943	4.546790
2.452613	253.441635	4.551795
2.336255	243.469301	4.556800
2.069333	238.729231	4.561805
2.289407	252.902144	4.566810
2.374816	264.686993	4.571814
2.353766	260.609891	4.576819
2.520648	268.234037	4.581824
2.293465	267.722242	4.586829
2.380959	257.959790	4.591834
2.204206	270.421132	4.596838
2.398956	260.283825	4.601843
2.503368	252.870704	4.606848
2.548308	267.130876	4.611853
2.588063	264.624270	4.616858
2.554452	254.314767	4.621862
2.537247	261.042076	4.626867
2.472258	262.939261	4.631872
2.600269	257.504308	4.636877
2.621431	258.065778	4.641882
2.433290	273.869153	4.646886
2.793610	265.184697	4.651891
2.705007	263.205599	4.656896
2.750861	277.040033	4.661901
2.996675	259.408863	4.666906
2.762330	263.831969	4.671910
2.624060	268.030841	4.676915
2.885858	264.076880	4.681920
2.631192	267.150100	4.686925
2.985920	261.661698	4.691930
2.894011	255.898066	4.696934
2.289044	238.089944	4.701939
2.366621	255.666409	4.706944
2.663423	252.240190	4.711949
2.672584	258.672012	4.716954
2.184253	262.415332	4.721958
2.452544	248.462251	4.726963
2.571818	264.579739	4.731968
2.329748	264.717677	4.736973
2.783101	251.943912	4.741978
2.427561	267.788459	4.746982
2.868767	279.336058	4.751987
2.889127	296.141467	4.756992
2.996794	290.832887	4.761997
3.287751	273.559264	4.767002
2.700875	278.387106	4.772006
2.709756	266.535110	4.777011
3.099283	282.992612	4.782016
2.864757	288.167899	4.787021
2.938947	278.898243	4.792026
3.181743	290.783875	4.797030
2.746807	284.136738	4.802035
3.100681	290.975878	4.807040
3.076703	302.527460	4.812045
3.260078	289.798870	4.817050
2.870213	266.828079	4.822054
2.890438	274.245020	4.827059
2.787252	277.093730	4.832064
2.794474	291.420731	4.837069
3.297967	297.176879	4.842074
3.122680	291.745075	4.847078
2.913223	294.274542	4.852083
3.186429	294.781931	4.857088
2.992300	290.875979	4.862093
3.333347	295.404279	4.867098
2.954528	301.427972	4.872102
3.064325	290.972907	4.877107
3.119741	298.474510	4.882112
3.067448	290.088979	4.887117
3.167149	293.012092	4.892122
2.879746	290.042694	4.897126
3.296407	290.012583	4.902131
3.072197	292.349052	4.907136
3.241782	303.233607	4.912141
3.328404	297.831820	4.917146
3.170221	300.863156	4.922150
2.882526	298.814550	4.927155
3.067144	297.474469	4.932160
2.992365	303.331803	4.937165
3.254048	312.025213	4.942170
3.502151	327.702392	4.947174
3.715435	312.830689	4.952179
3.491039	302.337021	4.957184
3.332253	305.160789	4.962189
3.675244	290.756904	4.967194
3.541661	300.964174	4.972198
3.541032	306.080887	4.977203
3.483119	299.333951	4.982208
3.340657	300.450363	4.987213
3.612810	296.797553	4.992218
3.218886	300.122967	4.997222
3.237818	290.791009	5.002227
3.158584	297.001669	5.007232
3.400111	308.093353	5.012237
3.609820	300.076206	5.017242
3.177974	312.890894	5.022246
3.312009	317.678047	5.027251
3.727470	324.904013	5.032256
3.869763	319.897899	5.037261
3.966701	327.647481	5.042266
3.598360	322.749920	5.047270
3.649761	296.041626	5.052275
3.803627	299.883146	5.057280
3.453339	296.414487	5.062285
3.561122	292.528983	5.067290
3.366854	295.229375	5.072294
3.557644	308.521850	5.077299
3.788643	317.497061	5.082304
3.631529	328.020974	5.087309
3.825908	323.566120	5.092314
3.370736	325.190884	5.097318
3.626941	332.111788	5.102323
3.512702	330.598623	5.107328
3.673476	324.613854	5.112333
3.617988	321.069146	5.117338
3.401157	336.848618	5.122342
3.933726	324.617722	5.127347
4.061156	328.379563	5.132352
3.790108	341.080688	5.137357
3.744817	323.364761	5.142362
3.528051	332.171184	5.147366
3.723735	340.288124	5.152371
3.839438	335.755899	5.157376
3.578382	337.315241	5.162381
4.048955	334.752230	5.167386
3.871423	326.964901	5.172390
3.780737	337.575019	5.177395
3.745825	321.241707	5.182400
3.856407	340.778516	5.187405
4.003355	332.717463	5.192410
3.599781	325.238001	5.197414
3.999376	348.030523	5.202419
3.997388	354.885485	5.207424
4.051875	347.646112	5.212429
4.257899	354.008940	5.217434
4.124778	345.289173	5.222438
4.239527	340.283559	5.227443
4.297227	339.688280	5.232448
3.696389	336.563690	5.237453
4.009736	331.738651	5.242458
3.898810	341.675244	5.247462
4.154838	332.555454	5.252467
4.223813	332.786028	5.257472
3.944516	335.599626	5.262477
4.132870	339.473143	5.267482
4.403805	344.543611	5.272486
4.155322	340.484143	5.277491
3.929088	335.012105	5.282496
4.088871	351.156336	5.287501
4.400512	360.428023	5.292506
4.277001	359.852428	5.297510
4.430806	352.914804	5.302515
3.967815	337.922598	5.307520
4.088803	355.603089	5.312525
4.390084	359.945700	5.317530
4.643657	360.462355	5.322534
4.178777	353.449389	5.327539
4.364689	337.359750	5.332544
3.852033	348.849663	5.337549
4.071799	356.775977	5.342554
3.886757	359.407178	5.347558
4.042726	362.781924	5.352563
4.426106	367.291312	5.357568
4.266113	362.988729	5.362573
4.405181	367.346804	5.367578
4.075649	362.328179	5.372582
4.177553	369.110042	5.377587
4.247134	369.541181	5.382592
4.206981	378.258857	5.387597
4.544927	363.664444	5.392602
3.896881	372.104427	5.397606
4.678826	380.657543	5.402611
4.826699	382.067626	5.407616
4.570276	391.477009	5.412621
4.662983	375.576759	5.417626
4.347435	376.711026	5.422630
4.442628	369.837636	5.427635
4.847961	371.466511	5.432640
4.498558	381.044661	5.437645
4.742302	365.273465	5.442650
4.526043	369.951695	5.447654
4.388135	366.085168	5.452659
4.789490	367.185907	5.457664
4.660751	367.495325	5.462669
4.673870	364.092974	5.467674
4.684346	361.017216	5.472678
4.488641	365.253032	5.477683
4.497320	374.175337	5.482688
4.909910	377.601697	5.487693
5.008417	387.452114	5.492698
4.645305	372.228597	5.497702
4.813723	375.929909	5.502707
4.833863	367.006631	5.507712
4.717760	372.954086	5.512717
4.728533	366.390712	5.517722
4.569998	375.709128	5.522726
4.598873	379.772777	5.527731
4.952318	373.197760	5.532736
5.102294	396.207211	5.537741
4.911144	380.748584	5.542746
4.755755	375.704927	5.547750
4.656865	367.724930	5.552755
4.878204	369.433636	5.557760
4.958322	390.996202	5.562765
5.065033	378.182735	5.567770
4.738337	378.299143	5.572774
4.857704	383.086964	5.577779
5.050427	385.140170	5.582784
4.763450	386.956260	5.587789
4.957915	379.333056	5.592794
4.961915	396.783131	5.597798
4.878120	393.273963	5.602803
4.594498	390.966786	5.607808
4.865687	400.450682	5.612813
4.808738	382.488888	5.617818
4.811952	386.739785	5.622822
4.896634	389.714529	5.627827
4.835126	388.254403	5.632832
4.720874	403.071183	5.637837
4.936417	391.174877	5.642842
5.120490	393.221522	5.647846
4.671289	393.310523	5.652851
5.081362	407.106788	5.657856
4.713451	413.706055	5.662861
5.145066	419.166322	5.667866
5.408249	430.388391	5.672870
5.501334	422.232802	5.677875
5.372671	415.550287	5.682880
5.222487	412.693938	5.687885
4.957066	394.160442	5.692890
5.085695	402.983228	5.697894
5.469268	418.077750	5.702899
5.226257	414.678153	5.707904
5.360044	419.204435	5.712909
5.138505	410.774293	5.717914
5.296326	409.266082	5.722918
5.573000	414.117695	5.727923
5.372983	399.782229	5.732928
5.072124	402.643600	5.737933
5.273042	391.480847	5.742938
5.411173	429.239230	5.747942
5.207429	417.671952	5.752947
5.215650	422.649024	5.757952
5.283742	430.614252	5.762957
5.342578	418.385701	5.767962
5.180787	426.720005	5.772966
5.387591	430.943189	5.777971
5.696643	429.751433	5.782976
5.330597	427.446624	5.787981
5.515755	426.890656	5.792986
5.015386	425.835617	5.797990
5.031894	429.450170	5.802995
5.411347	422.804933	5.808000
5.416185	425.394112	5.813005
5.261287	426.001947	5.818010
5.098198	426.869120	5.823014
5.548150	428.213898	5.828019
5.587645	417.946464	5.833024
5.578767	429.166038	5.838029
5.636420	428.322842	5.843034
5.388620	432.339588	5.848038
5.247288	437.817294	5.853043
5.577163	452.403866	5.858048
5.888236	460.463622	5.863053
5.773081	453.620713	5.868058
5.978131	461.142459	5.873062
5.654793	440.497868	5.878067
5.404410	439.794069	5.883072
5.498688	451.255584	5.888077
6.086747	451.056664	5.893082
5.692314	445.551215	5.898086
5.866891	455.751468	5.903091
5.812509	445.092179	5.908096
5.560581	436.335464	5.913101
5.518406	437.722303	5.918106
5.939297	454.957542	5.923110
5.938254	454.304683	5.928115
5.787696	456.012899	5.933120
5.799181	465.958743	5.938125
5.923497	464.848517	5.943130
5.921664	460.756051	5.948134
5.756566	454.112688	5.953139
5.573723	440.617361	5.958144
5.927865	456.652435	5.963149
5.969699	456.593699	5.968154
5.930866	461.870088	5.973158
5.911429	457.108193	5.978163
6.192565	457.600368	5.983168
5.991278	465.653143	5.988173
5.963047	456.625438	5.993178
5.932620	460.680262	5.998182
5.618395	459.486925	6.003187
6.019455	457.201258	6.008192
5.817688	463.423750	6.013197
6.118668	453.836032	6.018202
5.841082	466.045357	6.023206
6.300097	454.941325	6.028211
6.346589	458.056862	6.033216
6.187424	464.490541	6.038221
5.897007	432.979691	6.043226
5.941067	437.063437	6.048230
6.089779	457.191158	6.053235
6.033823	440.443488	6.058240
5.901087	436.573129	6.063245
5.894697	443.542904	6.068250
6.100411	453.417082	6.073254
6.082317	448.377843	6.078259
6.307002	451.573834	6.083264
5.873627	436.632674	6.088269
5.856263	423.452449	6.093274
6.067998	437.155436	6.098278
5.755387	441.191378	6.103283
5.773856	447.751670	6.108288
5.802539	450.349542	6.113293
5.877610	449.660033	6.118298
5.630384	464.798167	6.123302
5.735738	465.554192	6.128307
5.810631	462.575105	6.133312
5.753355	470.692086	6.138317
5.801094	453.850610	6.143322
6.357138	458.189922	6.148326
6.103498	460.659532	6.153331
6.415434	459.736331	6.158336
6.120507	462.402283	6.163341
6.178727	466.297336	6.168346
6.286489	460.686203	6.173350
6.019248	455.942369	6.178355
6.221511	463.210439	6.183360
6.196652	477.695635	6.188365
6.146012	470.801312	6.193370
6.117382	453.103890	6.198374
6.146887	444.221935	6.203379
5.750984	439.663630	6.208384
5.808570	450.595506	6.213389
6.087806	455.723735	6.218394
6.090724	461.701475	6.223398
6.092060	455.526453	6.228403
5.984635	435.691670	6.233408
5.822986	442.050968	6.238413
5.870518	451.907285	6.243418
5.858698	451.433196	6.248422
6.117033	463.925496	6.253427
6.459300	456.062365	6.258432
6.276057	445.571072	6.263437
6.097240	435.888623	6.268442
5.919726	434.625342	6.273446
5.928669	431.794982	6.278451
5.937284	422.584515	6.283456
5.873647	428.666766	6.288461
5.736199	432.577078	6.293466
5.828214	440.592718	6.298470
5.970464	447.007065	6.303475
6.157914	459.928389	6.308480
5.744682	449.327214	6.313485
6.028548	468.067218	6.318490
6.261436	467.150470	6.323494
5.773952	461.119857	6.328499
6.067265	459.310646	6.333504
6.118366	457.362303	6.338509
6.157417	451.606355	6.343514
6.002887	453.254554	6.348518
6.000640	450.269078	6.353523
5.895299	457.338181	6.358528
5.914931	462.617142	6.363533
6.164000	451.413339	6.368538
6.074981	459.655624	6.373542
5.769400	453.680588	6.378547
5.813421	449.028173	6.383552
5.821456	455.086752	6.388557
5.997279	450.288547	6.393562
5.874989	466.249446	6.398566
5.810076	454.277103	6.403571
6.268774	472.594289	6.408576
6.027517	465.416262	6.413581
6.073341	458.352594	6.418586
6.105457	473.336843	6.423590
5.475368	465.593547	6.428595
6.077805	456.241719	6.433600
5.663536	473.434943	6.438605
5.844706	464.052787	6.443610
5.865080	465.328367	6.448614
5.827818	459.910000	6.453619
6.084156	458.158793	6.458624
5.866067	461.770192	6.463629
5.897097	462.730483	6.468634
6.111316	468.511216	6.473638
6.022157	453.141619	6.478643
5.782440	462.819095	6.483648
5.824856	469.713237	6.488653
6.125608	455.673707	6.493658
6.060631	455.791951	6.498662
5.952817	456.374445	6.503667
6.311281	453.550547	6.508672
5.813216	460.832730	6.513677
6.162709	457.210412	6.518682
5.725697	456.575238	6.523686
6.099320	460.684639	6.528691
6.019797	458.536004	6.533696
6.022568	463.457263	6.538701
6.064067	459.268254	6.543706
5.861120	463.122608	6.548710
5.818785	456.915833	6.553715
5.792837	458.181309	6.558720
5.443861	464.070894	6.563725
6.109329	481.540701	6.568730
6.178155	493.030722	6.573734
5.898472	495.944253	6.578739
5.793235	486.546667	6.583744
6.293966	503.698524	6.588749
6.424443	476.144487	6.593754
6.107503	471.068005	6.598758
5.868831	468.127909	6.603763
6.194982	465.814665	6.608768
6.068446	461.025972	6.613773
6.004716	459.893053	6.618778
6.134084	458.164505	6.623782
6.322740	467.500088	6.628787
5.746979	459.627951	6.633792
5.501722	454.195320	6.638797
5.952517	456.662961	6.643802
6.070895	465.668215	6.648806
5.997366	463.553217	6.653811
6.010935	459.949118	6.658816
6.025594	463.486540	6.663821
6.039470	462.615455	6.668826
6.019620	456.079498	6.673830
6.128151	459.058898	6.678835
6.558772	454.678322	6.683840
6.219849	472.037562	6.688845
6.098815	460.511140	6.693850
6.014191	464.013569	6.698854
6.112963	456.194919	6.703859
6.319071	462.753017	6.708864
6.107278	468.656733	6.713869
6.213394	472.895483	6.718874
6.096372	469.682133	6.723878
6.011549	478.602488	6.728883
6.243592	470.809458	6.733888
5.871796	470.660041	6.738893
6.037125	469.288801	6.743898
5.591389	470.839113	6.748902
5.714688	453.200344	6.753907
5.901091	457.954913	6.758912
5.907737	477.632293	6.763917
6.217082	465.923759	6.768922
5.864752	453.068982	6.773926
5.999241	453.973700	6.778931
6.249105	461.073291	6.783936
5.810152	458.740866	6.788941
6.520066	454.600929	6.793946
6.137517	460.988945	6.798950
5.911046	460.190430	6.803955
6.216072	467.656788	6.808960
5.889265	468.098483	6.813965
5.833510	452.804165	6.818970
6.010760	459.755144	6.823974
5.798387	462.220105	6.828979
6.015715	453.218021	6.833984
5.754957	461.035561	6.838989
5.985328	458.975215	6.843994
6.064495	456.875039	6.848998
6.009240	459.692085	6.854003
6.018026	463.813929	6.859008
5.722278	461.647750	6.864013
6.098810	461.988312	6.869018
6.203906	471.930332	6.874022
5.956357	463.572828	6.879027
5.918563	457.682975	6.884032
6.061796	471.722087	6.889037
6.237752	468.960705	6.894042
6.019724	464.482802	6.899046
6.005044	462.905620	6.904051
6.367145	468.482855	6.909056
5.967018	472.403436	6.914061
6.016794	458.870737	6.919066
6.028760	472.725154	6.924070
6.064324	469.854082	6.929075
6.091413	464.952889	6.934080
5.998565	470.683145	6.939085
6.113854	463.741279	6.944090
6.210312	461.666757	6.949094
6.135957	458.405416	6.954099
5.868948	439.877158	6.959104
5.812975	436.427213	6.964109
6.130057	453.929401	6.969114
6.081880	459.133934	6.974118
5.759332	449.924409	6.979123
6.014147	451.119416	6.984128
5.884755	468.567445	6.989133
5.779033	459.265948	6.994138
6.028604	450.018409	6.999142
5.804607	472.494977	7.004147
5.950909	462.855962	7.009152
6.081165	458.501441	7.014157
6.069794	461.344680	7.019162
6.320180	466.854545	7.024166
5.957439	459.859477	7.029171
6.454712	455.707917	7.034176
5.925929	449.410461	7.039181
6.042102	437.132366	7.044186
5.936220	443.581895	7.049190
6.201602	446.196884	7.054195
6.126938	431.730179	7.059200
5.611320	438.267738	7.064205
5.734418	441.240584	7.069210
6.056673	454.422177	7.074214
5.908956	462.058946	7.079219
6.294675	464.469270	7.084224
5.761815	461.632840	7.089229
6.066954	459.014670	7.094234
6.008124	460.692142	7.099238
5.892555	465.029380	7.104243
5.920105	461.348485	7.109248
5.640142	469.644725	7.114253
6.093373	466.023513	7.119258
6.005339	460.621428	7.124262
5.990467	465.411135	7.129267
6.422971	462.174655	7.134272
5.767509	465.851919	7.139277
6.096727	461.928498	7.144282
6.156480	465.578335	7.149286
5.927220	461.811132	7.154291
6.093824	463.465261	7.159296
5.825825	474.259862	7.164301
6.179910	457.923486	7.169306
5.995107	465.305736	7.174310
6.035809	471.438440	7.179315
6.338496	458.626064	7.184320
6.004718	460.993983	7.189325
5.932141	439.527884	7.194330
6.042489	458.940279	7.199334
5.897962	452.150368	7.204339
6.060132	448.209371	7.209344
5.862774	467.740009	7.214349
6.104862	459.917700	7.219354
6.287218	463.129666	7.224358
5.787298	445.559857	7.229363
6.094641	433.686922	7.234368
6.067109	439.590071	7.239373
6.283801	434.429857	7.244378
5.924143	446.748524	7.249382
5.968305	433.889016	7.254387
5.969469	436.606859	7.259392
6.089368	445.706066	7.264397
6.159021	436.276256	7.269402
6.252577	442.116579	7.274406
6.276760	437.302296	7.279411
6.382376	428.867114	7.284416
5.810511	444.993442	7.289421
6.319575	439.604273	7.294426
5.917741	431.239923	7.299430
5.942580	435.663755	7.304435
6.008493	445.332150	7.309440
6.065975	444.269274	7.314445
5.701228	435.197746	7.319450
5.971911	443.692137	7.324454
5.851022	443.938303	7.329459
5.901115	437.120776	7.334464
5.724406	439.915664	7.339469
5.794667	436.759866	7.344474
5.677229	438.334059	7.349478
5.688228	447.738253	7.354483
6.097386	444.534639	7.359488
6.084456	468.769491	7.364493
6.269919	459.757475	7.369498
6.093189	449.791432	7.374502
5.909538	441.357282	7.379507
5.950887	422.365214	7.384512
5.747947	441.399615	7.389517
6.044077	451.951612	7.394522
6.350694	453.650576	7.399526
5.929327	442.102569	7.404531
5.937235	440.358973	7.409536
5.686386	439.720857	7.414541
5.753835	450.418966	7.419546
5.986460	458.054541	7.424550
6.010705	467.535384	7.429555
6.204315	465.688586	7.434560
5.980807	473.030965	7.439565
6.136584	472.221866	7.444570
6.073110	469.423099	7.449574
6.159134	464.610230	7.454579
6.244572	457.645972	7.459584
5.867208	451.221681	7.464589
5.879926	428.599659	7.469594
5.631329	455.728629	7.474598
5.892472	462.687548	7.479603
6.293491	461.265521	7.484608
6.029609	478.933296	7.489613
6.195417	468.842366	7.494618
6.113418	458.933569	7.499622
5.501732	450.969111	7.504627
5.833281	451.508695	7.509632
5.860963	465.855959	7.514637
6.158098	474.245958	7.519642
6.069823	473.366595	7.524646
5.996513	471.718499	7.529651
6.284137	472.614091	7.534656
6.014089	471.322591	7.539661
5.987690	474.550904	7.544666
6.033955	472.095082	7.549670
6.086511	463.784372	7.554675
5.890733	465.570108	7.559680
6.093319	475.386907	7.564685
5.933847	465.495249	7.569690
6.074521	467.742245	7.574694
5.742502	468.884271	7.579699
6.213872	465.602793	7.584704
5.905493	465.944957	7.589709
5.892594	472.543197	7.594714
5.870720	473.711023	7.599718
5.995800	470.642053	7.604723
6.056316	471.059303	7.609728
5.669609	485.986200	7.614733
5.570091	462.007904	7.619738
5.591357	467.368481	7.624742
5.630832	471.202310	7.629747
6.036776	471.750812	7.634752
5.874284	474.111343	7.639757
5.896492	476.444805	7.644762
5.953006	463.577113	7.649766
5.500468	468.558816	7.654771
6.024645	470.810313	7.659776
5.676730	478.289668	7.664781
5.971683	492.383540	7.669786
6.056293	493.870582	7.674790
5.942101	498.681448	7.679795
6.189552	504.000419	7.684800
6.064392	510.557638	7.689805
5.767602	500.216975	7.694810
6.170076	506.501527	7.699814
5.950849	501.763754	7.704819
6.141647	482.270012	7.709824
6.215082	504.685637	7.714829
5.989969	492.075684	7.719834
6.084426	475.604514	7.724838
5.707283	483.555640	7.729843
6.044186	482.219876	7.734848
5.982032	504.602265	7.739853
6.080388	486.541582	7.744858
5.971961	497.487607	7.749862
6.092643	501.562951	7.754867
6.087762	491.534348	7.759872
5.760041	491.442465	7.764877
5.972445	495.016473	7.769882
6.179706	496.150776	7.774886
6.247680	502.216240	7.779891
6.333751	481.341847	7.784896
5.590163	464.880826	7.789901
5.887872	462.646273	7.794906
5.917679	476.812853	7.799910
5.974502	489.060263	7.804915
6.134165	487.959979	7.809920
6.064435	482.647500	7.814925
6.060475	476.340159	7.819930
6.129759	468.268390	7.824934
6.073443	481.645949	7.829939
5.997426	472.428424	7.834944
5.627916	479.208622	7.839949
5.591557	476.580684	7.844954
6.254079	492.597491	7.849958
6.021120	498.271591	7.854963
6.184749	504.433027	7.859968
6.203932	501.756838	7.864973
5.776302	476.193667	7.869978
5.745322	482.843044	7.874982
5.598018	500.408017	7.879987
6.176412	493.106565	7.884992
5.963894	506.665637	7.889997
6.078967	504.528544	7.895002
6.110502	509.200989	7.900006
6.023672	515.085453	7.905011
6.238510	503.621193	7.910016
5.831117	504.799257	7.915021
6.093142	504.984219	7.920026
6.152506	495.793242	7.925030
5.566891	501.893312	7.930035
5.726322	504.341530	7.935040
5.928270	509.368798	7.940045
6.053071	500.166413	7.945050
6.065394	513.001689	7.950054
6.090544	501.764017	7.955059
6.134588	498.035499	7.960064
5.898501	506.210362	7.965069
5.993075	498.836238	7.970074
6.038256	508.735796	7.975078
5.632649	508.806642	7.980083
6.089827	502.723002	7.985088
6.331564	505.985838	7.990093
6.137262	508.253763	7.995098
5.927792	502.163577	8.000102
6.175703	509.663762	8.005107
6.435164	511.815958	8.010112
6.336001	496.100500	8.015130
6.155493	479.492184	8.020147
6.227723	473.411330	8.025165
6.197853	474.977029	8.030182
6.034054	471.808783	8.035200
5.764905	478.819471	8.040218
5.996507	457.103496	8.045235
5.951347	461.103486	8.050253
5.702235	469.014898	8.055270
5.945573	461.735647	8.060288
5.748235	470.946100	8.065306
5.915035	487.767103	8.070323
5.960247	492.798303	8.075341
6.375147	496.711255	8.080358
6.550581	496.622898	8.085376
5.912930	492.905722	8.090394
5.926662	476.095860	8.095411
6.239154	469.142114	8.100429
5.721787	474.246988	8.105446
5.984624	492.926434	8.110464
6.345192	493.194508	8.115482
6.161613	493.042178	8.120499
6.334423	499.640149	8.125517
5.609701	495.950547	8.130534
5.917678	485.790147	8.135552
6.094387	506.416799	8.140570
5.803615	503.445181	8.145587
6.118896	504.546451	8.150605
5.964782	514.136910	8.155622
6.021821	496.782382	8.160640
6.190441	512.281146	8.165658
5.944708	511.085962	8.170675
6.306466	500.620171	8.175693
5.816156	510.981290	8.180710
6.218146	509.893295	8.185728
6.049494	514.715013	8.190746
6.240046	502.405957	8.195763
6.256794	505.747931	8.200781
6.005034	514.640011	8.205798
6.148096	504.747744	8.210816
5.906420	512.876014	8.215834
6.261019	512.778026	8.220851
6.147722	498.642216	8.225869
6.255743	497.504200	8.230886
6.502476	512.194750	8.235904
6.382852	507.326737	8.240922
6.139759	500.694367	8.245939
6.217684	505.602670	8.250957
6.163974	517.931276	8.255974
6.418920	495.775162	8.260992
6.187870	499.923572	8.266010
5.950396	517.474266	8.271027
5.906189	508.386699	8.276045
6.494091	525.617190	8.281062
6.662655	528.441467	8.286080
6.265720	520.292509	8.291098
6.250581	500.813639	8.296115
6.339137	505.882554	8.301133
6.347518	509.301288	8.306150
6.214848	499.319087	8.311168
6.433595	508.086473	8.316186
6.276027	507.918135	8.321203
6.621554	505.777784	8.326221
6.344967	501.247949	8.331238
6.529284	496.473973	8.336256
6.584286	509.159430	8.341274
6.351571	511.364529	8.346291
6.395388	495.382767	8.351309
6.347279	502.892652	8.356326
6.566763	504.484555	8.361344
6.296625	505.496287	8.366362
6.417401	494.283087	8.371379
6.844886	501.457544	8.376397
6.307203	510.229189	8.381414
6.428897	500.655253	8.386432
6.335312	505.615516	8.391450
6.215507	510.909375	8.396467
6.297553	506.224919	8.401485
6.123367	507.470153	8.406502
6.217183	511.585742	8.411520
6.293221	505.477677	8.416538
6.311313	501.359580	8.421555
6.701596	508.601002	8.426573
6.565587	502.401136	8.431590
6.516141	502.686780	8.436608
6.554214	502.425494	8.441626
6.351401	509.883012	8.446643
6.721713	504.161660	8.451661
6.410875	504.319767	8.456678
6.511708	500.674115	8.461696
6.417094	507.195047	8.466714
6.460726	508.878498	8.471731
6.673950	503.685361	8.476749
6.500254	514.395947	8.481766
6.238165	508.316302	8.486784
6.246909	515.171659	8.491802
6.413552	521.066475	8.496819
6.464190	503.363661	8.501837
6.501876	510.387719	8.506854
6.619042	507.993828	8.511872
6.624991	515.255565	8.516890
6.332407	514.071665	8.521907
6.253777	506.102842	8.526925
6.245096	513.203841	8.531942
6.782946	526.686600	8.536960
6.764859	522.998994	8.541978
6.407202	517.856500	8.546995
6.599542	504.752824	8.552013
6.552854	507.398737	8.557030
6.443423	512.763505	8.562048
6.524453	525.887002	8.567066
6.757947	534.480447	8.572083
7.148844	522.450800	8.577101
6.557880	520.720269	8.582119
6.743218	501.959095	8.587136
6.548314	503.812054	8.592154
6.335231	509.925489	8.597171
6.009613	511.743269	8.602189
5.987332	533.869168	8.607207
6.191728	533.758411	8.612224
6.639297	537.296169	8.617242
6.522865	529.505199	8.622259
6.464936	534.030633	8.627277
6.593465	534.834390	8.632295
6.758538	539.280661	8.637312
6.642014	541.677544	8.642330
6.458738	544.732371	8.647347
6.764758	530.680061	8.652365
6.683147	529.938854	8.657383
6.495676	536.480260	8.662400
6.652510	535.706046	8.667418
6.919483	534.724104	8.672435
6.700070	535.433225	8.677453
6.556141	543.945472	8.682471
6.689103	543.295945	8.687488
6.893055	538.596550	8.692506
6.377038	550.106587	8.697523
6.822724	538.316543	8.702541
6.711540	541.233597	8.707559
6.692380	541.883254	8.712576
6.999424	549.087772	8.717594
6.386825	539.787189	8.722611
6.930124	529.541918	8.727629
6.752160	548.792300	8.732647
7.100494	546.706390	8.737664
7.300159	540.527400	8.742682
7.005858	558.530649	8.747699
7.109392	535.483350	8.752717
7.004214	550.034691	8.757735
6.963905	542.695605	8.762752
7.174643	541.270785	8.767770
6.605836	552.221949	8.772787
7.023568	545.944040	8.777805
6.919188	550.833774	8.782823
6.791806	555.964762	8.787840
7.367842	539.501778	8.792858
6.969943	540.625944	8.797875
6.915530	528.818570	8.802893
6.581863	518.748928	8.807911
6.681404	531.575830	8.812928
7.054788	539.861279	8.817946
6.798918	543.655707	8.822963
7.205869	539.519591	8.827981
6.831968	536.340194	8.832999
6.820480	537.966333	8.838016
6.954515	533.617694	8.843034
6.532140	543.757613	8.848051
6.657012	531.441183	8.853069
6.765101	535.942135	8.858087
6.733841	550.299704	8.863104
7.056060	544.879236	8.868122
6.634638	542.728837	8.873139
7.046122	554.053133	8.878157
6.953742	540.600496	8.883175
7.139423	536.788976	8.888192
6.926978	552.142035	8.893210
6.553443	547.452653	8.898227
6.997368	536.896700	8.903245
6.913883	547.448042	8.908263
6.558768	541.164904	8.913280
7.025854	531.562016	8.918298
7.062049	542.918897	8.923315
7.034413	533.124885	8.928333
6.984562	548.378055	8.933351
6.989484	543.640599	8.938368
7.037635	529.863827	8.943386
6.821414	553.808832	8.948403
6.725765	536.855790	8.953421
7.002548	537.597163	8.958439
6.898701	542.954918	8.963456
7.477415	552.100253	8.968474
7.037422	546.188053	8.973491
7.077754	530.702692	8.978509
6.881753	541.873974	8.983527
6.848023	546.417062	8.988544
6.800656	558.384785	8.993562
7.120868	582.002458	8.998579
7.258010	569.119125	9.003597
7.336792	574.164682	9.008615
7.021753	583.555642	9.013632
7.278719	560.096515	9.018650
7.035537	572.896050	9.023667
7.368611	566.500063	9.028685
6.907363	551.006248	9.033703
6.773721	567.216395	9.038720
7.180024	567.730306	9.043738
7.008543	569.181747	9.048755
6.934745	571.435481	9.053773
7.159075	562.335684	9.058791
7.264708	574.864531	9.063808
7.175335	567.222582	9.068826
7.048653	574.004694	9.073843
7.290894	573.652298	9.078861
7.169885	573.912178	9.083879
6.899399	581.509529	9.088896
7.285603	563.514332	9.093914
7.070685	573.999438	9.098931
7.029479	583.013128	9.103949
7.193136	567.594733	9.108967
7.223382	573.451295	9.113984
6.879967	571.930094	9.119002
6.959107	578.984235	9.124019
7.024208	563.609586	9.129037
6.985824	572.493894	9.134055
6.782232	579.854349	9.139072
7.319564	592.688862	9.144090
7.312016	608.279814	9.149107
7.377329	606.780320	9.154125
7.712081	609.484944	9.159143
7.744967	599.858902	9.164160
7.325261	583.941640	9.169178
6.904764	574.965025	9.174195
7.117872	575.851343	9.179213
7.290736	590.344376	9.184231
7.499722	602.420036	9.189248
7.580676	591.096736	9.194266
7.329626	578.176876	9.199283
7.289498	573.753484	9.204301
7.220284	573.049195	9.209319
7.194863	566.916148	9.214336
7.642063	578.992475	9.219354
7.361007	578.521774	9.224371
7.199092	581.428620	9.229389
7.516789	581.105872	9.234407
7.381247	596.208127	9.239424
7.523950	573.941341	9.244442
7.525889	562.081627	9.249459
7.725661	577.273402	9.254477
7.567286	568.117578	9.259495
7.226829	574.552911	9.264512
7.640650	573.565593	9.269530
7.076051	567.293248	9.274547
7.382860	566.081440	9.279565
7.626388	563.940717	9.284583
7.704150	581.377396	9.289600
7.678169	571.308536	9.294618
7.514755	569.150037	9.299635
7.324878	572.955610	9.304653
7.254133	573.293485	9.309671
7.140229	565.976882	9.314688
7.397554	575.307597	9.319706
7.529499	581.623045	9.324723
7.653667	583.613602	9.329741
7.719244	579.798990	9.334759
7.339857	584.292932	9.339776
7.301144	584.903016	9.344794
7.755140	585.247564	9.349811
7.644955	570.859650	9.354829
7.733856	577.002325	9.359847
7.370483	583.548218	9.364864
7.643968	561.536652	9.369882
7.547499	579.000546	9.374899
7.275042	577.939962	9.379917
7.358357	585.688353	9.384935
7.398715	600.147693	9.389952
7.682515	609.875153	9.394970
7.760654	605.688358	9.399987
7.739462	602.080364	9.405005
7.909090	601.062546	9.410023
7.631990	584.070259	9.415040
7.521192	579.383404	9.420058
7.655296	569.508321	9.425075
7.303893	581.045399	9.430093
7.754319	583.449169	9.435111
7.832809	597.232264	9.440128
7.446872	590.118347	9.445146
7.609513	596.017101	9.450163
7.745225	605.078226	9.455181
8.175461	604.900430	9.460199
7.412358	596.832508	9.465216
7.642471	578.652599	9.470234
7.524392	578.777574	9.475251
7.443272	600.897351	9.480269
7.627804	599.466032	9.485287
7.780520	608.760522	9.490304
7.874798	607.712448	9.495322
7.908715	611.037338	9.500339
7.752855	613.063545	9.505357
7.876125	602.697713	9.510375
7.506257	605.048793	9.515392
7.752175	607.421119	9.520410
7.687274	608.634525	9.525427
7.736445	611.016731	9.530445
7.572411	594.964706	9.535463
7.492033	596.341757	9.540480
7.604877	606.078178	9.545498
7.752084	613.992170	9.550515
7.526371	607.978113	9.555533
7.848133	607.717574	9.560551
7.422046	616.140197	9.565568
7.796060	610.714393	9.570586
7.834962	606.167424	9.575603
7.792410	600.951477	9.580621
8.173396	604.421038	9.585639
7.971578	604.626668	9.590656
7.882919	595.423192	9.595674
8.000849	601.123670	9.600691
7.631716	600.128558	9.605709
8.155839	605.546800	9.610727
8.030351	611.954004	9.615744
7.945123	608.876563	9.620762
7.974758	608.163416	9.625779
7.635609	603.364024	9.630797
8.019978	603.461962	9.635815
7.766868	602.434687	9.640832
7.708437	598.628755	9.645850
8.076867	604.056783	9.650867
7.666451	598.305489	9.655885
7.958948	600.279646	9.660903
7.691303	605.326173	9.665920
7.851567	599.197559	9.670938
8.083998	607.012934	9.675955
7.703797	598.543321	9.680973
7.896429	605.415072	9.685991
8.152678	608.881630	9.691008
7.893521	623.555218	9.696026
7.938051	624.037397	9.701043
8.147065	634.637491	9.706061
8.239285	626.021698	9.711079
7.907781	613.945348	9.716096
7.873655	608.881912	9.721114
8.166591	615.294367	9.726131
8.125816	635.615371	9.731149
8.387780	625.319499	9.736167
8.065915	617.459599	9.741184
8.273274	608.715263	9.746202
8.149281	591.804830	9.751219
7.988046	603.408905	9.756237
8.053720	606.784145	9.761255
7.931516	608.215737	9.766272
7.891541	601.964535	9.771290
8.172850	604.304542	9.776307
7.822497	609.622953	9.781325
7.982839	621.877793	9.786343
8.197943	635.689419	9.791360
8.258452	633.334294	9.796378
8.555476	631.163368	9.801395
7.940847	617.752880	9.806413
8.202302	613.490326	9.811431
8.516227	607.242044	9.816448
8.144507	610.642823	9.821466
8.475907	602.959368	9.826483
8.317921	604.058260	9.831501
8.239538	600.337793	9.836519
8.023213	604.023556	9.841536
7.972337	613.970169	9.846554
8.171434	605.465046	9.851571
7.994743	605.080423	9.856589
7.911847	606.922560	9.861607
8.171609	623.248526	9.866624
8.058128	631.080139	9.871642
8.381479	631.444112	9.876659
8.000173	641.554380	9.881677
8.601411	632.846694	9.886695
8.351977	648.099585	9.891712
8.246388	636.158193	9.896730
8.368110	633.561405	9.901747
8.035193	647.231070	9.906765
8.321861	644.481261	9.911783
8.113565	642.539477	9.916800
8.103391	627.979403	9.921818
8.389022	628.555080	9.926835
8.050710	643.381700	9.931853
8.061014	631.286246	9.936871
8.198301	640.673641	9.941888
8.165071	637.121554	9.946906
8.599274	636.039052	9.951923
8.586567	637.597503	9.956941
8.787729	642.391016	9.961959
8.720981	635.556942	9.966976
8.985545	641.737432	9.971994
8.770337	640.379842	9.977011
8.487578	629.087490	9.982029
8.049219	617.347432	9.987047
8.264678	620.733940	9.992064
8.177125	637.287655	9.997082
8.430635	631.028288	10.002099
8.322464	631.930307	10.007117
8.393645	629.195937	10.012135
8.284270	635.271520	10.017152
8.284753	634.229693	10.022170
8.536183	628.091907	10.027187
8.470227	642.386314	10.032205
8.627593	636.503095	10.037223
8.616083	643.583957	10.042240
8.319782	645.953194	10.047258
8.804251	631.231176	10.052275
8.213061	629.356604	10.057293
8.646222	629.692492	10.062311
8.919458	633.101437	10.067328
8.443493	638.942286	10.072346
8.572724	639.482207	10.077363
8.301988	632.941829	10.082381
8.507576	632.465004	10.087399
8.564834	633.600066	10.092416
8.529458	631.386746	10.097434
8.743284	632.463462	10.102451
8.559892	632.342786	10.107469
8.728459	637.717552	10.112487
8.755749	638.324407	10.117504
8.577532	646.152850	10.122522
8.749338	629.713861	10.127539
8.405196	643.005042	10.132557
8.483546	638.180142	10.137575
8.506225	634.767310	10.142592
8.471698	636.211477	10.147610
8.587542	647.785444	10.152627
8.633018	649.386830	10.157645
8.411912	641.175097	10.162663
8.739569	638.683718	10.167680
8.397515	649.767819	10.172698
8.670607	633.138994	10.177715
8.454282	645.116894	10.182733
8.412645	661.640316	10.187751
8.653057	661.032956	10.192768
8.543278	665.167963	10.197786
8.828799	670.696903	10.202803
8.836308	674.161183	10.207821
8.818945	669.057858	10.212839
8.989590	670.487017	10.217856
9.157965	667.860471	10.222874
9.139758	666.907442	10.227891
8.694206	652.823345	10.232909
8.634750	646.264678	10.237927
9.105580	633.548643	10.242944
8.806873	640.359704	10.247962
8.797202	627.588065	10.252979
8.759425	637.624341	10.257997
8.516580	644.966615	10.263015
8.600656	650.924131	10.268032
8.699318	666.679542	10.273050
8.685199	660.966849	10.278067
8.719928	668.963223	10.283085
8.770631	666.154785	10.288103
8.878446	664.533028	10.293120
8.952108	670.001131	10.298138
8.846212	667.295524	10.303155
8.903669	668.768087	10.308173
8.962495	667.845922	10.313191
9.056792	669.003306	10.318208
8.735320	669.316979	10.323226
9.201251	660.994261	10.328243
9.003463	677.101171	10.333261
8.948645	668.299261	10.338279
9.149280	666.716289	10.343296
8.832144	668.275356	10.348314
9.244561	663.520317	10.353331
9.550763	662.278687	10.358349
9.068147	665.275250	10.363367
9.260954	669.969188	10.368384
9.074136	664.352144	10.373402
9.186140	644.901480	10.378419
9.087143	654.551310	10.383437
8.996483	654.120094	10.388455
9.117353	635.589740	10.393472
8.745619	649.218686	10.398490
9.156296	646.142540	10.403507
8.928661	652.128737	10.408525
8.733754	670.730431	10.413543
8.894275	670.752981	10.418560
8.808044	673.023151	10.423578
8.959643	655.143274	10.428595
9.117223	650.689945	10.433613
9.149073	664.484350	10.438631
9.285357	663.749148	10.443648
8.837337	678.603673	10.448666
8.603474	662.129345	10.453683
8.896948	667.410168	10.458701
8.920671	671.189816	10.463719
9.074346	664.199839	10.468736
8.856407	671.285993	10.473754
9.165690	681.323496	10.478771
8.975191	697.233100	10.483789
9.273020	704.529452	10.488807
9.539614	690.571191	10.493824
9.230747	691.243242	10.498842
9.287804	682.475385	10.503859
9.150472	678.277434	10.508877
9.020305	680.926248	10.513895
9.413884	687.011043	10.518912
9.394611	699.633748	10.523930
9.466144	679.936825	10.528947
9.388563	669.738856	10.533965
8.897717	668.299083	10.538983
9.192754	683.973744	10.544000
8.934647	690.992150	10.549018
9.228429	692.619227	10.554035
9.231597	700.427859	10.559053
9.043193	699.126551	10.564071
9.286418	702.871803	10.569088
9.029539	693.037831	10.574106
9.200857	693.129745	10.579123
9.291369	693.482600	10.584141
9.028566	700.120267	10.589159
9.308698	698.663990	10.594176
8.978212	704.341185	10.599194
9.528510	697.858667	10.604211
9.218942	696.722039	10.609229
9.253170	718.237507	10.614247
9.787918	720.164956	10.619264
9.635830	714.876833	10.624282
9.231854	708.932147	10.629299
9.359966	703.194556	10.634317
9.324974	722.249515	10.639335
9.911383	724.532726	10.644352
9.383665	709.100119	10.649370
10.017171	700.634258	10.654387
9.846997	703.609309	10.659405
9.681382	702.071407	10.664423
9.521258	692.692022	10.669440
9.586822	700.700538	10.674458
9.386884	693.748711	10.679475
9.212861	690.595000	10.684493
9.353939	689.454459	10.689511
9.516752	687.440814	10.694528
9.359059	700.854746	10.699546
9.409003	693.612561	10.704563
9.545120	692.332906	10.709581
9.159197	699.068659	10.714599
9.716043	714.086626	10.719616
9.729893	726.603604	10.724634
9.756223	724.838153	10.729651
9.484202	711.788503	10.734669
9.370736	725.178812	10.739687
9.739947	718.423317	10.744704
9.559731	725.609836	10.749722
9.547758	728.607853	10.754739
9.946092	723.821468	10.759757
9.429684	730.327862	10.764775
10.009264	726.052463	10.769792
9.865928	728.876853	10.774810
9.871800	723.338258	10.779827
9.747347	709.035627	10.784845
9.340606	714.297854	10.789863
9.711194	707.050894	10.794880
9.771326	714.677221	10.799898
9.638138	728.601988	10.804915
9.964248	724.948676	10.809933
9.840895	725.247029	10.814951
9.779018	704.811738	10.819968
9.548838	711.942248	10.824986
9.600437	712.559751	10.830003
9.889536	729.735932	10.835021
9.520836	732.544622	10.840039
10.020363	728.028269	10.845056
10.200899	719.098675	10.850074
9.801652	722.573305	10.855091
9.985161	711.532517	10.860109
9.647713	718.345093	10.865127
9.667929	721.217538	10.870144
9.642394	726.901424	10.875162
9.782786	718.346109	10.880179
10.071943	722.995408	10.885197
9.939188	721.271204	10.890215
10.113328	730.804207	10.895232
9.964922	732.218983	10.900250
9.763631	727.156660	10.905267
9.893413	725.906686	10.910285
9.505949	737.209139	10.915303
9.551813	715.256126	10.920320
9.573244	724.102591	10.925338
9.554989	733.747295	10.930355
9.629915	721.989252	10.935373
9.682057	731.354461	10.940391
9.909040	749.022921	10.945408
10.018113	753.790455	10.950426
9.776727	763.543789	10.955443
9.959220	760.581592	10.960461
9.845689	757.002696	10.965479
10.022018	755.723378	10.970496
10.026907	762.200618	10.975514
10.032142	769.111677	10.980531
10.297331	760.472047	10.985549
9.926681	765.436750	10.990567
10.193813	753.853475	10.995584
10.170417	757.411250	11.000602
9.940208	772.718654	11.005619
10.258616	752.506131	11.010637
9.793035	761.109438	11.015655
9.821939	767.246655	11.020672
9.932081	759.389195	11.025690
9.795133	762.263903	11.030707
9.879697	760.144993	11.035725
10.032299	762.917041	11.040743
10.047873	759.106122	11.045760
10.049410	760.295865	11.050778
9.699902	765.125210	11.055795
10.393331	774.005411	11.060813
10.556029	788.754593	11.065831
10.221309	771.018123	11.070848
10.547383	772.525229	11.075866
10.335680	760.589861	11.080883
10.302311	766.180389	11.085901
10.126265	773.586769	11.090919
10.148753	765.521097	11.095936
10.239573	761.100909	11.100954
10.192671	776.031931	11.105971
10.415625	758.496767	11.110989
10.173037	756.513696	11.116007
10.183382	764.613638	11.121024
10.405458	770.258590	11.126042
10.098494	764.536289	11.131059
10.165505	767.800637	11.136077
10.214119	787.935450	11.141095
10.307124	784.830292	11.146112
10.582711	789.147862	11.151130
10.705132	798.731375	11.156147
10.600317	778.438096	11.161165
10.146294	764.105442	11.166183
10.374593	778.504764	11.171200
10.635396	785.603868	11.176218
10.229120	778.993127	11.181235
10.496056	786.049296	11.186253
10.380299	785.365383	11.191271
10.382483	778.077320	11.196288
10.807247	796.089358	11.201306
10.344807	780.793107	11.206323
10.545544	765.499267	11.211341
10.338263	766.322316	11.216359
10.294616	779.350809	11.221376
10.610110	785.883404	11.226394
10.325750	790.092363	11.231411
10.612596	785.484392	11.236429
10.343500	797.188507	11.241447
10.336766	792.566756	11.246464
10.893756	799.398066	11.251482
11.051579	803.511620	11.256499
11.181115	785.888043	11.261517
10.845081	773.489248	11.266535
10.516149	765.164190	11.271552
10.617591	746.405168	11.276570
10.564343	745.910888	11.281587
10.254610	750.124817	11.286605
10.199317	752.727615	11.291623
10.460057	773.637926	11.296640
10.710575	772.076813	11.301658
10.585176	789.511186	11.306675
10.672446	791.587773	11.311693
10.720359	786.148684	11.316711
10.963596	795.140982	11.321728
10.964166	790.458784	11.326746
10.830077	777.834426	11.331763
10.605055	763.749505	11.336781
10.597960	764.300445	11.341799
10.741757	769.728653	11.346816
11.071039	774.192335	11.351834
10.633984	766.685580	11.356851
10.574277	758.910410	11.361869
10.556501	768.945336	11.366887
10.766273	776.647635	11.371904
11.032493	780.165330	11.376922
10.597191	795.362090	11.381939
10.704397	780.789167	11.386957
10.893638	786.264387	11.391975
10.511924	786.298310	11.396992
10.867828	773.711071	11.402010
10.733558	782.734944	11.407027
10.601936	785.991773	11.412045
10.951162	779.535266	11.417063
10.844680	791.114885	11.422080
11.271552	778.022704	11.427098
11.042320	781.480863	11.432115
11.057525	789.872085	11.437133
11.295922	788.176090	11.442151
11.225251	795.258827	11.447168
11.006950	775.615384	11.452186
10.879857	763.875735	11.457203
10.913715	767.928579	11.462221
10.526788	779.211096	11.467239
10.679061	788.223440	11.472256
10.948801	791.192138	11.477274
10.787827	789.159854	11.482291
10.705195	783.901265	11.487309
10.672920	792.300236	11.492327
10.734931	790.222542	11.497344
11.044035	783.948121	11.502362
10.830041	788.721916	11.507379
10.895698	790.369480	11.512397
10.745026	796.812118	11.517415
11.248482	806.763592	11.522432
11.476715	806.592016	11.527450
11.187763	799.095311	11.532467
11.007290	793.909372	11.537485
11.349774	790.810221	11.542503
10.986013	794.584259	11.547520
11.001609	794.887697	11.552538
11.197884	783.006425	11.557555
10.970579	784.660774	11.562573
11.037025	801.223561	11.567591
10.816424	816.804664	11.572608
11.363670	812.562237	11.577626
11.250206	826.745298	11.582643
11.225701	832.781545	11.587661
11.101801	821.466342	11.592679
11.130338	806.309067	11.597696
11.067345	816.750239	11.602714
11.026923	824.733232	11.607731
11.079009	816.958255	11.612749
11.338934	827.462881	11.617767
11.275208	827.211622	11.622784
11.164157	822.108967	11.627802
11.282714	830.211136	11.632819
11.268277	810.625380	11.637837
11.215326	816.379171	11.642855
11.090534	817.261216	11.647872
11.200285	820.683737	11.652890
11.256519	827.997832	11.657907
10.932870	820.279040	11.662925
11.301850	828.392079	11.667943
10.898623	842.359702	11.672960
11.468635	840.788101	11.677978
11.138068	856.788227	11.682995
11.373154	851.017945	11.688013
11.576503	840.860726	11.693031
11.553018	857.313063	11.698048
11.632709	838.655831	11.703066
11.588760	855.331684	11.708083
11.904786	853.246743	11.713101
11.799794	844.703272	11.718119
11.684541	844.849136	11.723136
11.488306	821.277924	11.728154
11.255782	826.373827	11.733171
11.640369	837.478018	11.738189
11.771197	841.502556	11.743207
11.144546	833.051791	11.748224
11.194567	838.773223	11.753242
11.346368	849.937736	11.758259
11.451564	859.304293	11.763277
11.693196	846.966151	11.768295
11.348934	847.990350	11.773312
11.698914	843.583897	11.778330
11.570579	847.601076	11.783347
11.619949	841.229914	11.788365
11.806426	834.945428	11.793383
11.409770	852.033038	11.798400
11.328953	843.227354	11.803418
11.344889	845.885412	11.808435
11.492276	847.788816	11.813453
11.673990	853.664836	11.818471
11.625296	847.225739	11.823488
11.828492	843.680884	11.828506
11.721228	858.037818	11.833523
11.990378	843.561082	11.838541
11.988592	851.380450	11.843559
11.673749	849.775970	11.848576
11.834241	849.687129	11.853594
11.718858	854.335516	11.858611
11.448161	849.323985	11.863629
11.983030	853.630217	11.868647
11.659461	844.354211	11.873664
11.534101	849.924250	11.878682
11.630258	870.754627	11.883699
11.929040	872.307781	11.888717
12.071662	871.223261	11.893735
11.948242	874.333407	11.898752
12.045824	863.817539	11.903770
12.153987	853.856617	11.908787
11.930015	853.169622	11.913805
12.100344	858.752207	11.918823
11.776509	842.700646	11.923840
12.067447	851.993009	11.928858
11.841576	847.006053	11.933875
11.791600	852.240074	11.938893
12.057232	847.239798	11.943911
11.830099	858.520962	11.948928
11.906995	838.037763	11.953946
12.052185	850.446344	11.958963
12.038351	859.613911	11.963981
12.245041	846.946271	11.968999
11.962061	853.844967	11.974016
12.200324	853.789033	11.979034
11.995616	854.220791	11.984051
11.788466	857.393776	11.989069
12.297980	856.098557	11.994087
11.871028	857.681497	11.999104
11.900726	865.486715	12.004122
12.255950	874.190525	12.009139
12.368085	873.681999	12.014157
12.486705	869.251380	12.019175
12.260343	867.081592	12.024192
12.272090	853.758001	12.029210
12.003644	849.799739	12.034227
11.939108	855.242624	12.039245
12.097208	850.324081	12.044263
12.069429	871.688230	12.049280
12.316402	890.812628	12.054298
12.230348	880.212353	12.059315
11.898311	877.384758	12.064333
12.158828	875.350023	12.069351
12.026281	877.615280	12.074368
12.097358	878.548410	12.079386
12.550818	887.539579	12.084403
12.049104	872.567384	12.089421
12.205561	871.894378	12.094439
12.415244	881.647052	12.099456
12.270593	869.235053	12.104474
11.869694	877.598252	12.109491
11.983773	878.611760	12.114509
12.101952	875.325684	12.119527
12.078535	883.860814	12.124544
12.188904	891.291659	12.129562
12.199200	905.206651	12.134579
12.408219	901.452493	12.139597
12.579298	898.243679	12.144615
12.453101	914.810671	12.149632
12.503096	910.045578	12.154650
12.719611	905.780235	12.159667
12.476282	910.337696	12.164685
12.494170	903.020409	12.169703
12.788925	905.734058	12.174720
12.685214	897.002585	12.179738
12.762615	887.079987	12.184755
12.569785	880.197556	12.189773
12.522182	870.830171	12.194791
12.557769	882.471997	12.199808
12.845577	872.583227	12.204826
12.730090	867.181149	12.209843
12.291497	863.911704	12.214861
12.688480	872.985412	12.219879
12.815797	881.533322	12.224896
12.745268	872.290962	12.229914
12.526185	878.870211	12.234931
12.516306	883.639827	12.239949
12.803307	860.618012	12.244967
12.717381	882.998094	12.249984
12.741586	878.072540	12.255002
12.512405	875.070989	12.260019
12.600769	887.932117	12.265037
12.472848	881.272578	12.270055
12.126968	884.425884	12.275072
12.555741	889.990472	12.280090
12.807663	895.397707	12.285107
12.726555	900.270323	12.290125
13.022115	901.763689	12.295143
12.924376	903.922134	12.300160
12.604403	903.708200	12.305178
12.743809	902.393641	12.310195
12.571927	905.083239	12.315213
12.990506	898.500970	12.320231
12.653490	901.620734	12.325248
12.898907	892.641645	12.330266
13.119582	895.311048	12.335283
12.630828	899.458063	12.340301
13.136634	897.085306	12.345319
12.838746	901.688388	12.350336
12.570440	896.878968	12.355354
13.046559	886.213245	12.360371
13.004910	895.417117	12.365389
12.954300	907.033055	12.370407
12.817609	905.367344	12.375424
12.860437	889.769713	12.380442
12.955894	900.975557	12.385459
12.807563	900.996793	12.390477
13.027808	890.601458	12.395495
12.687914	892.977148	12.400512
12.858272	897.241089	12.405530
12.722260	895.343419	12.410547
12.554731	906.271427	12.415565
13.061694	910.438809	12.420583
13.303427	920.757760	12.425600
13.219612	908.357917	12.430618
13.031018	909.413374	12.435635
12.609603	909.144563	12.440653
13.021422	913.602323	12.445671
13.308525	922.168232	12.450688
13.267797	930.933963	12.455706
13.627250	922.228971	12.460723
13.234122	916.579010	12.465741
13.358777	897.900400	12.470759
13.135944	902.186608	12.475776
12.952521	891.736741	12.480794
13.188602	900.412232	12.485811
12.797196	912.094134	12.490829
13.511347	920.059648	12.495847
13.432508	917.985433	12.500864
13.353772	920.378000	12.505882
13.158944	916.842317	12.510899
13.149394	926.695508	12.515917
13.408711	925.366741	12.520935
13.488774	928.316130	12.525952
13.353225	928.747384	12.530970
13.250930	916.595819	12.535987
13.017424	930.353127	12.541005
13.631049	922.203464	12.546023
13.310487	925.113072	12.551040
13.272717	925.885779	12.556058
13.281830	923.253132	12.561075
13.704308	930.543263	12.566093
13.414338	921.713249	12.571111
13.696590	924.232546	12.576128
13.791999	930.726684	12.581146
13.888305	911.298353	12.586163
13.565647	899.998026	12.591181
13.648080	898.080889	12.596199
13.476972	886.038143	12.601216
13.326176	887.720109	12.606234
13.525850	892.225024	12.611251
13.416991	891.453761	12.616269
13.671804	887.539311	12.621287
13.537704	902.202634	12.626304
13.032023	893.397162	12.631322
13.979081	901.284619	12.636339
13.508616	920.304621	12.641357
13.760353	914.351085	12.646375
13.892432	924.937031	12.651392
13.468342	915.958054	12.656410
13.601895	909.476414	12.661427
13.537588	927.968861	12.666445
13.544048	915.477238	12.671463
13.884084	907.803030	12.676480
13.641454	918.477068	12.681498
13.781983	918.012954	12.686515
13.684757	919.393113	12.691533
13.415925	918.569165	12.696551
13.754686	930.848596	12.701568
13.525755	927.465272	12.706586
14.006111	911.501179	12.711603
13.830407	919.660780	12.716621
13.812504	918.882949	12.721639
13.868140	905.890089	12.726656
13.714797	915.737217	12.731674
14.229770	914.631903	12.736691
13.897121	910.492144	12.741709
13.655075	912.626316	12.746727
14.117721	924.292958	12.751744
13.920266	928.563171	12.756762
13.819495	923.672031	12.761779
13.859159	926.106735	12.766797
13.977512	918.731409	12.771815
13.710563	923.027275	12.776832
13.479742	924.581254	12.781850
14.017356	919.794821	12.786867
13.819942	915.390040	12.791885
13.523263	921.031321	12.796903
13.898455	924.525728	12.801920
13.885403	939.525415	12.806938
14.138689	941.593187	12.811955
14.107834	943.692366	12.816973
14.410983	941.188555	12.821991
14.184326	935.156123	12.827008
13.947206	934.290818	12.832026
13.731622	912.119456	12.837043
14.079937	926.671003	12.842061
14.165301	951.894893	12.847079
14.453262	950.709494	12.852096
14.419803	947.503865	12.857114
14.486342	933.621939	12.862131
14.153491	920.060015	12.867149
14.090449	918.931046	12.872167
14.141448	906.584602	12.877184
14.043074	921.984127	12.882202
14.266692	936.626257	12.887219
14.168504	940.261382	12.892237
14.334691	944.944552	12.897255
14.505396	944.219197	12.902272
14.321911	945.027302	12.907290
14.510408	927.710002	12.912307
14.138744	916.332640	12.917325
14.187659	922.296466	12.922343
14.448918	921.375375	12.927360
14.709173	943.987852	12.932378
14.551406	932.305988	12.937395
14.275925	922.095189	12.942413
14.176736	913.211216	12.947431
14.471890	908.305432	12.952448
14.005299	924.323284	12.957466
14.522358	932.499886	12.962483
14.489483	941.487021	12.967501
14.529510	946.721454	12.972519
14.734867	939.907620	12.977536
14.141017	952.558664	12.982554
14.186020	954.719507	12.987571
14.468249	944.197083	12.992589
14.118897	952.605043	12.997607
14.709679	952.275442	13.002624
14.470178	956.930987	13.007642
14.800885	943.616017	13.012659
14.368971	957.812361	13.017677
14.633179	947.479690	13.022695
14.647651	952.038255	13.027712
14.408714	958.390644	13.032730
14.763404	944.145401	13.037747
14.956646	945.638261	13.042765
14.865936	953.573933	13.047783
14.675553	946.489923	13.052800
14.992157	944.175291	13.057818
14.794609	941.727650	13.062835
14.735035	944.913563	13.067853
14.639270	937.540448	13.072871
14.526836	943.780112	13.077888
14.532620	950.177475	13.082906
14.439413	940.363335	13.087923
14.446842	948.095911	13.092941
14.471661	941.443678	13.097959
14.561203	956.029847	13.102976
14.690229	981.449487	13.107994
15.102437	978.308960	13.113011
14.940984	966.469144	13.118029
15.070309	991.596284	13.123047
14.832270	972.822920	13.128064
14.963403	968.094884	13.133082
15.016054	979.243796	13.138099
15.082903	975.898674	13.143117
14.890248	969.545607	13.148135
15.256305	968.384597	13.153152
14.704334	967.023977	13.158170
14.976932	970.776054	13.163187
15.229633	973.414100	13.168205
14.889596	980.945299	13.173223
15.162861	967.576820	13.178240
15.335827	973.794034	13.183258
14.691028	963.631050	13.188275
15.081762	952.035566	13.193293
14.848888	969.138261	13.198311
14.734097	968.103160	13.203328
14.928759	969.996208	13.208346
14.893479	965.401461	13.213363
15.123445	970.746123	13.218381
14.896485	973.624822	13.223399
15.218829	968.674573	13.228416
15.067731	979.584467	13.233434
14.893602	965.100076	13.238451
15.224232	974.710503	13.243469
15.158125	969.930332	13.248487
15.279837	962.571455	13.253504
15.063479	973.311452	13.258522
15.096095	971.751885	13.263539
15.450935	977.218506	13.268557
15.326876	995.169531	13.273575
15.259762	1005.472363	13.278592
15.623329	1009.361063	13.283610
15.518406	985.876951	13.288627
15.332660	982.612440	13.293645
14.890959	976.226818	13.298663
15.618277	987.862073	13.303680
15.641715	997.656619	13.308698
15.353427	988.346157	13.313715
15.530339	983.639582	13.318733
15.351045	987.187451	13.323751
15.641449	987.727714	13.328768
15.526800	996.045150	13.333786
15.326808	974.012830	13.338803
15.720207	978.956834	13.343821
15.597071	995.190002	13.348839
15.745465	992.701916	13.353856
15.484785	981.434488	13.358874
15.292057	968.971014	13.363891
15.439038	984.572829	13.368909
15.428766	998.710458	13.373927
15.697987	992.746918	13.378944
15.448504	1000.082978	13.383962
15.586383	1006.986592	13.388979
15.739269	989.558003	13.393997
15.229962	990.383048	13.399015
15.655857	991.867384	13.404032
15.592991	987.280042	13.409050
15.552760	994.971707	13.414067
15.841456	989.168602	13.419085
15.837850	984.433207	13.424103
15.640940	993.777341	13.429120
15.796777	1000.746870	13.434138
15.166545	1000.410416	13.439155
15.175233	995.229462	13.444173
15.740594	1019.546930	13.449191
15.980533	1014.726700	13.454208
15.524316	1019.008404	13.459226
15.894708	1029.782954	13.464243
16.468461	1023.204119	13.469261
16.131624	1021.576586	13.474279
15.939321	997.463014	13.479296
16.063992	1009.865471	13.484314
16.172645	995.975250	13.489331
16.203156	988.514228	13.494349
16.075375	999.981109	13.499367
15.938079	987.584529	13.504384
15.927232	1002.593656	13.509402
16.170908	996.896198	13.514419
16.320027	984.378288	13.519437
16.188145	1000.624027	13.524455
16.167941	997.112020	13.529472
16.434342	1001.483029	13.534490
16.001811	998.744347	13.539507
16.537993	992.470893	13.544525
16.121859	999.976888	13.549543
16.202028	992.560011	13.554560
16.129735	993.165131	13.559578
16.069355	986.565829	13.564595
16.182153	984.739610	13.569613
15.962083	991.211708	13.574631
16.064245	987.955514	13.579648
15.852027	986.518575	13.584666
15.870825	999.037614	13.589683
16.368788	994.047905	13.594701
15.870892	996.560135	13.599719
16.152623	999.397092	13.604736
16.178172	1018.593962	13.609754
16.171555	1021.450133	13.614771
16.439448	1024.838400	13.619789
16.612010	1032.786502	13.624807
16.404577	1027.926437	13.629824
16.436529	1032.318288	13.634842
16.432280	1040.200156	13.639859
16.650602	1010.873351	13.644877
16.389001	1014.875890	13.649895
16.160872	1013.782167	13.654912
16.294818	1011.334450	13.659930
16.399696	1021.825074	13.664947
16.461115	1012.672715	13.669965
16.395125	1021.591956	13.674983
16.785228	1026.268950	13.680000
16.747504	1029.045435	13.685018
16.508453	1022.966502	13.690035
16.656545	1017.109273	13.695053
16.531827	1018.829947	13.700071
16.650116	1018.094849	13.705088
16.463412	1015.960900	13.710106
16.479270	1019.217222	13.715123
16.566084	1022.466445	13.720141
16.634904	1018.847217	13.725159
16.673482	1022.769746	13.730176
16.681342	1017.727381	13.735194
16.904673	1023.877839	13.740211
17.012784	1028.834167	13.745229
16.480873	1016.371006	13.750247
16.569574	1014.368778	13.755264
16.650303	1023.968179	13.760282
16.487783	1023.791697	13.765299
16.987825	1014.058972	13.770317
16.593642	1028.658621	13.775335
16.984253	1016.298873	13.780352
16.879336	1016.408883	13.785370
16.713443	1028.361329	13.790387
16.723230	1011.148552	13.795405
16.828938	1022.615934	13.800423
16.891618	1009.797185	13.805440
16.968451	1009.190078	13.810458
16.828835	1028.539822	13.815475
16.662354	1017.456865	13.820493
16.664499	1029.048826	13.825511
16.699948	1051.907630	13.830528
17.112683	1051.804266	13.835546
16.949541	1055.917591	13.840563
17.060691	1046.060954	13.845581
17.018249	1052.796979	13.850599
17.414242	1043.767924	13.855616
17.113135	1053.235397	13.860634
17.231194	1056.358520	13.865651
17.278330	1045.240735	13.870669
17.393693	1054.201766	13.875687
17.336281	1051.558146	13.880704
17.347499	1035.367664	13.885722
17.153232	1030.656478	13.890739
17.280261	1024.653738	13.895757
16.681494	1029.748527	13.900775
17.281786	1028.102133	13.905792
17.401982	1036.440614	13.910810
17.076149	1058.809916	13.915827
17.527178	1041.038547	13.920845
17.332191	1048.263281	13.925863
17.297202	1058.379671	13.930880
17.301431	1051.184235	13.935898
16.916417	1057.951189	13.940915
17.138754	1061.779691	13.945933
16.890302	1055.428035	13.950951
16.999476	1054.946759	13.955968
17.227773	1050.381942	13.960986
17.009076	1071.520187	13.966003
17.257858	1056.654066	13.971021
17.465146	1077.542725	13.976039
17.396466	1092.930134	13.981056
17.816043	1095.380712	13.986074
17.636212	1081.077635	13.991091
17.733847	1080.693426	13.996109
17.191727	1072.688124	14.001127
17.270422	1081.382149	14.006144
17.773582	1085.272205	14.011162
17.754672	1086.816965	14.016179
17.759034	1087.872629	14.021197
17.797800	1092.786214	14.026215
17.526121	1089.884738	14.031232
17.612806	1097.160077	14.036250
17.637260	1084.521273	14.041267
17.409651	1090.451051	14.046285
17.689410	1088.144355	14.051303
17.673754	1080.931821	14.056320
17.674102	1082.964554	14.061338
17.350393	1099.243966	14.066355
17.668789	1083.056502	14.071373
17.235189	1094.693555	14.076391
17.890841	1088.125368	14.081408
17.818562	1086.155834	14.086426
17.952261	1095.408297	14.091443
17.744838	1082.555986	14.096461
17.727448	1092.644102	14.101479
17.459892	1105.188602	14.106496
18.112387	1098.780551	14.111514
17.988690	1114.903031	14.116531
18.124197	1121.735447	14.121549
18.056683	1106.485302	14.126567
18.169178	1109.903990	14.131584
18.162320	1099.408960	14.136602
17.918414	1090.793442	14.141619
17.712821	1104.676388	14.146637
18.077105	1114.186082	14.151655
17.991372	1120.798604	14.156672
18.094027	1118.072527	14.161690
17.810710	1121.957541	14.166707
18.020953	1114.125773	14.171725
17.807815	1124.766739	14.176743
17.777623	1124.264601	14.181760
18.369611	1115.908016	14.186778
17.863697	1122.426616	14.191795
18.083829	1123.057519	14.196813
18.249416	1121.637550	14.201831
18.258168	1115.883414	14.206848
18.483903	1113.607981	14.211866
18.643773	1127.391291	14.216883
18.314872	1112.934796	14.221901
18.498738	1125.610390	14.226919
18.220154	1120.887819	14.231936
18.565241	1115.621712	14.236954
18.169798	1123.512569	14.241971
18.329365	1119.888458	14.246989
18.332783	1116.951850	14.252007
18.385308	1106.601503	14.257024
18.650256	1119.720505	14.262042
18.182532	1121.009077	14.267059
18.551506	1111.292341	14.272077
18.545511	1104.434536	14.277095
18.483293	1121.035363	14.282112
18.442952	1102.573994	14.287130
18.329054	1106.083233	14.292147
18.504509	1123.208076	14.297165
18.779620	1107.370890	14.302183
18.183445	1120.493437	14.307200
18.626631	1103.923875	14.312218
18.377842	1120.889531	14.317235
18.633505	1135.953451	14.322253
18.576124	1140.121552	14.327271
18.655721	1154.149017	14.332288
18.793536	1148.553433	14.337306
18.610400	1154.248955	14.342323
18.807684	1148.826189	14.347341
18.662268	1146.178693	14.352359
18.593603	1154.683563	14.357376
18.709724	1153.724051	14.362394
18.686910	1150.817161	14.367411
18.644383	1150.662869	14.372429
18.652020	1149.147759	14.377447
18.654812	1151.146834	14.382464
18.969494	1161.326651	14.387482
18.856709	1149.910468	14.392499
18.985050	1149.736994	14.397517
18.859500	1161.170658	14.402535
18.465368	1164.201701	14.407552
18.603193	1156.517682	14.412570
18.475400	1169.117078	14.417587
18.758586	1179.803406	14.422605
19.068418	1178.510948	14.427623
18.821059	1186.130950	14.432640
19.137631	1188.182885	14.437658
19.064352	1179.752570	14.442675
19.010326	1188.567192	14.447693
19.195529	1177.046638	14.452711
18.895036	1187.813088	14.457728
19.250638	1172.200684	14.462746
19.314637	1186.096132	14.467763
19.145402	1188.432250	14.472781
19.564511	1183.145622	14.477799
19.118485	1190.154468	14.482816
19.637514	1176.229336	14.487834
19.321144	1177.874926	14.492851
19.018650	1187.366130	14.497869
19.167842	1177.453230	14.502887
18.969697	1182.920770	14.507904
19.343337	1184.319287	14.512922
19.347366	1183.168292	14.517939
19.137040	1168.969861	14.522957
19.361504	1181.861589	14.527975
19.316396	1176.365305	14.532992
19.361507	1171.347340	14.538010
19.425298	1191.619324	14.543027
19.238446	1187.950491	14.548045
19.593782	1175.771810	14.553063
19.058059	1184.065539	14.558080
19.411655	1207.379888	14.563098
19.638201	1208.185691	14.568115
19.357389	1203.965742	14.573133
19.747745	1214.012242	14.578151
19.581459	1213.953978	14.583168
19.759615	1219.332777	14.588186
20.191915	1216.711828	14.593203
19.830298	1191.049320	14.598221
19.911021	1189.973235	14.603239
19.750191	1185.795658	14.608256
19.672467	1170.542610	14.613274
19.912380	1171.671541	14.618291
19.817193	1179.208332	14.623309
19.531076	1179.515285	14.628327
19.720878	1182.720264	14.633344
19.499290	1172.028030	14.638362
19.442561	1184.298032	14.643379
19.542712	1190.631484	14.648397
19.915604	1198.428871	14.653415
20.001649	1216.245449	14.658432
19.987751	1218.649391	14.663450
20.282171	1204.026039	14.668467
20.011342	1207.167007	14.673485
20.000980	1205.649552	14.678503
19.827473	1210.470813	14.683520
19.850972	1207.414353	14.688538
20.140924	1209.767295	14.693555
19.808387	1208.630781	14.698573
20.044070	1214.893625	14.703591
20.050965	1220.884488	14.708608
20.023559	1219.670192	14.713626
20.114912	1215.727858	14.718643
19.927779	1223.648308	14.723661
19.963459	1210.747549	14.728679
19.920033	1213.868457	14.733696
19.986169	1211.925436	14.738714
20.101436	1213.858500	14.743731
20.096659	1208.184899	14.748749
19.842370	1212.425907	14.753767
19.962650	1223.191144	14.758784
19.855726	1228.095487	14.763802
20.307893	1235.249581	14.768819
20.414291	1246.951622	14.773837
20.292786	1242.046389	14.778855
20.105090	1241.090432	14.783872
20.154541	1251.827046	14.788890
20.310867	1252.159887	14.793907
20.108469	1246.363836	14.798925
20.361900	1243.441392	14.803943
20.187411	1248.952479	14.808960
20.371571	1243.959142	14.813978
20.216069	1241.915363	14.818995
20.309241	1264.085821	14.824013
20.552231	1282.406574	14.829031
20.316375	1291.735674	14.834048
20.526823	1290.456481	14.839066
20.562995	1279.362973	14.844083
20.202225	1284.317548	14.849101
20.703098	1281.955489	14.854119
20.120419	1291.844577	14.859136
20.139953	1276.452144	14.864154
20.588142	1277.193769	14.869171
20.522602	1298.187743	14.874189
20.730040	1278.979818	14.879207
20.553453	1278.897079	14.884224
20.723298	1300.697694	14.889242
21.026193	1299.871062	14.894259
20.625061	1313.501219	14.899277
21.054366	1324.513446	14.904295
21.255274	1311.850415	14.909312
20.477096	1285.380740	14.914330
20.820254	1291.657937	14.919347
20.892459	1305.562963	14.924365
20.831416	1300.443224	14.929383
20.878649	1315.339236	14.934400
21.242509	1317.207222	14.939418
21.218172	1309.428880	14.944435
20.669761	1316.999694	14.949453
21.136563	1310.756079	14.954471
20.894227	1302.625047	14.959488
20.871039	1309.854578	14.964506
20.891130	1308.452534	14.969523
20.691212	1302.566498	14.974541
20.819190	1298.479333	14.979559
20.633071	1309.327738	14.984576
20.930597	1311.213573	14.989594
21.136428	1311.349289	14.994611
21.064626	1341.034325	14.999629
21.456960	1333.256988	15.004647
21.018709	1337.091293	15.009664
21.289638	1338.761482	15.014682
21.764996	1346.034808	15.019699
21.150214	1342.510853	15.024717
21.280699	1332.871572	15.029735
21.076404	1343.506897	15.034752
21.527725	1343.652628	15.039770
21.687075	1339.725793	15.044787
21.414495	1342.805473	15.049805
21.359603	1334.906400	15.054823
21.632564	1337.965407	15.059840
21.359812	1338.276846	15.064858
21.798416	1346.367536	15.069875
21.417981	1341.236597	15.074893
21.674138	1334.345801	15.079911
21.595115	1342.272261	15.084928
21.359233	1333.295986	15.089946
21.692559	1332.140950	15.094963
21.391180	1346.954859	15.099981
21.320528	1338.211866	15.104999
21.438476	1334.966966	15.110016
21.749092	1341.904774	15.115034
22.182384	1340.180351	15.120051
21.733487	1342.118484	15.125069
21.845943	1336.987580	15.130087
21.907800	1347.590145	15.135104
21.669144	1343.770805	15.140122
21.604586	1334.886081	15.145139
21.534211	1348.372256	15.150157
21.605812	1346.922726	15.155175
21.728995	1335.268034	15.160192
21.474665	1352.805242	15.165210
21.260691	1346.363332	15.170227
21.441370	1348.081108	15.175245
21.518391	1356.443923	15.180263
21.669435	1374.830759	15.185280
21.582551	1372.179062	15.190298
21.883809	1369.050493	15.195315
21.848754	1382.455085	15.200333
21.833092	1369.029689	15.205351
22.006741	1384.111145	15.210368
22.157198	1405.941289	15.215386
22.445790	1397.441805	15.220403
22.091986	1391.675639	15.225421
22.207317	1384.420749	15.230439
22.110107	1381.623141	15.235456
22.031324	1376.266386	15.240474
22.195673	1389.328434	15.245491
22.256684	1386.858169	15.250509
22.396749	1396.839669	15.255527
22.634484	1407.336255	15.260544
22.474823	1391.014409	15.265562
22.678575	1383.774628	15.270579
22.076466	1373.327981	15.275597
21.975785	1367.493818	15.280615
22.419953	1375.131508	15.285632
22.472884	1388.571754	15.290650
22.457667	1398.716494	15.295667
22.436376	1394.936210	15.300685
22.409432	1390.629777	15.305703
22.610124	1413.227299	15.310720
22.189357	1410.346166	15.315738
22.484700	1396.401314	15.320755
22.382203	1400.497229	15.325773
22.417818	1407.316559	15.330791
22.573203	1412.268348	15.335808
22.334555	1404.129566	15.340826
22.835648	1392.033306	15.345843
22.718893	1409.438413	15.350861
22.667342	1402.218375	15.355879
22.712181	1406.385402	15.360896
22.732230	1409.672999	15.365914
22.803872	1389.180488	15.370931
22.742672	1394.348153	15.375949
22.338951	1402.642622	15.380967
22.628257	1392.263781	15.385984
22.544585	1404.842695	15.391002
22.658548	1428.053103	15.396019
22.719601	1438.438376	15.401037
23.157973	1431.415473	15.406055
23.199228	1429.209647	15.411072
22.852556	1437.358114	15.416090
22.842501	1427.400316	15.421107
22.863096	1441.024665	15.426125
22.920955	1427.538848	15.431143
23.244227	1432.691016	15.436160
22.945449	1442.603550	15.441178
23.437631	1424.551754	15.446195
23.384836	1424.799096	15.451213
22.965643	1424.313599	15.456231
22.818424	1427.581604	15.461248
23.024854	1427.609955	15.466266
23.164380	1419.587583	15.471283
22.719154	1429.038752	15.476301
23.051867	1439.186053	15.481319
22.874525	1430.353174	15.486336
22.855901	1442.628304	15.491354
23.130495	1464.272097	15.496371
23.390433	1464.576603	15.501389
23.248943	1451.507115	15.506407
23.421250	1462.244437	15.511424
23.720965	1469.593886	15.516442
23.742933	1465.028599	15.521459
23.579713	1465.264469	15.526477
23.555585	1465.463576	15.531495
24.188602	1454.467742	15.536512
23.434083	1450.509835	15.541530
23.351536	1437.616221	15.546547
23.505960	1436.051043	15.551565
23.445784	1452.426332	15.556583
23.484423	1465.827872	15.561600
23.328865	1466.737179	15.566618
23.436847	1465.673694	15.571635
23.772856	1474.658048	15.576653
23.364633	1468.556408	15.581671
23.763156	1470.071098	15.586688
23.405568	1477.849595	15.591706
23.456895	1458.629454	15.596723
23.436482	1463.088734	15.601741
23.429989	1465.757790	15.606759
23.944517	1468.402550	15.611776
23.731258	1483.362633	15.616794
23.791578	1495.656645	15.621811
23.760235	1496.419461	15.626829
23.773370	1501.728202	15.631847
23.778871	1497.390200	15.636864
23.800170	1496.550062	15.641882
23.728646	1498.377435	15.646899
23.964263	1492.786230	15.651917
23.734597	1489.219465	15.656935
24.253136	1482.596813	15.661952
23.520709	1492.700116	15.666970
23.442202	1494.420981	15.671987
23.931539	1518.326274	15.677005
24.139491	1531.841014	15.682023
24.694448	1517.575633	15.687040
24.612984	1532.549216	15.692058
24.183081	1530.742053	15.697075
24.414338	1522.983366	15.702093
24.189781	1531.613993	15.707111
24.320019	1520.438045	15.712128
24.376669	1535.900743	15.717146
24.368659	1526.831195	15.722163
24.345341	1530.108664	15.727181
24.297584	1524.795344	15.732199
24.453907	1517.483626	15.737216
24.476880	1521.763927	15.742234
24.533640	1524.778198	15.747251
24.740637	1522.355234	15.752269
24.949070	1532.273367	15.757287
24.722281	1514.773874	15.762304
24.503750	1507.095623	15.767322
24.617052	1496.856213	15.772339
24.701615	1494.751276	15.777357
24.398966	1502.549443	15.782375
24.940132	1504.235222	15.787392
24.543624	1515.791079	15.792410
24.791323	1514.225831	15.797427
24.937965	1509.299033	15.802445
24.433251	1517.797431	15.807463
24.958218	1519.624255	15.812480
25.139344	1517.001658	15.817498
24.688680	1512.354639	15.822515
24.725261	1508.138252	15.827533
24.748101	1516.290257	15.832551
24.964808	1518.455380	15.837568
24.850943	1529.724418	15.842586
24.797324	1524.361287	15.847603
24.835249	1516.354473	15.852621
24.688998	1519.588680	15.857639
24.714415	1517.773986	15.862656
24.386890	1514.134225	15.867674
24.853386	1532.295328	15.872691
24.745443	1530.923081	15.877709
25.060825	1545.961592	15.882727
25.312661	1548.337025	15.887744
25.039637	1554.474653	15.892762
25.314116	1559.230260	15.897779
25.271792	1550.470656	15.902797
25.554400	1544.983463	15.907815
25.379979	1535.708175	15.912832
24.909092	1532.510938	15.917850
24.855334	1528.473819	15.922867
25.375725	1542.020588	15.927885
25.061917	1556.038045	15.932903
25.346517	1549.604986	15.937920
25.378149	1549.859438	15.942938
25.326968	1547.979259	15.947955
25.394813	1541.376146	15.952973
25.294295	1544.703377	15.957991
25.652450	1540.395264	15.963008
25.707673	1535.530802	15.968026
25.821355	1541.784417	15.973043
26.012362	1551.150797	15.978061
25.603028	1552.625986	15.983079
25.091239	1538.503797	15.988096
25.530962	1558.791296	15.993114
25.460940	1545.740032	15.998131
25.274484	1539.228344	16.003149
25.550897	1556.845379	16.008167
25.669800	1540.992032	16.013184
25.506325	1540.653224	16.018202
25.662996	1567.747764	16.023219
26.086393	1568.270699	16.028237
25.948195	1580.358247	16.033255
26.003825	1577.906948	16.038272
25.777750	1578.146514	16.043290
26.026464	1588.445571	16.048307
26.233744	1579.215040	16.053325
25.730900	1575.304081	16.058343
25.872051	1576.945553	16.063360
26.223841	1573.669243	16.068378
25.778816	1577.061284	16.073395
26.314146	1578.506338	16.078413
26.255812	1577.733677	16.083431
26.548169	1576.141362	16.088448
26.393146	1563.951647	16.093466
25.578509	1549.300244	16.098483
26.050268	1559.014274	16.103501
26.249282	1584.959686	16.108519
26.318234	1576.359804	16.113536
25.979767	1582.116186	16.118554
26.036729	1583.709375	16.123571
26.338766	1577.976474	16.128589
26.563187	1584.568647	16.133607
26.151442	1580.443645	16.138624
26.064830	1580.086230	16.143642
26.301735	1591.690010	16.148659
26.488688	1582.793695	16.153677
26.146072	1572.025133	16.158695
26.073706	1572.414864	16.163712
26.319649	1590.900434	16.168730
26.193338	1604.596244	16.173747
26.672245	1606.033895	16.178765
26.568459	1621.330894	16.183783
26.601669	1611.536277	16.188800
26.647635	1599.961655	16.193818
26.404039	1619.249117	16.198835
26.647421	1619.762633	16.203853
26.657925	1619.329138	16.208871
26.433234	1613.960785	16.213888
26.787099	1613.604390	16.218906
26.592726	1610.472451	16.223923
26.556052	1609.262608	16.228941
26.455001	1626.316003	16.233959
27.018460	1632.518359	16.238976
27.012053	1633.142041	16.243994
26.879769	1643.924509	16.249011
26.985359	1638.194328	16.254029
26.848467	1639.687094	16.259047
27.224491	1641.647586	16.264064
27.352245	1639.024735	16.269082
27.207193	1639.800051	16.274099
27.258619	1620.750928	16.279117
26.871637	1610.366783	16.284135
27.014054	1623.967423	16.289152
27.111031	1628.895671	16.294170
27.145275	1637.633571	16.299187
27.581054	1641.733107	16.304205
27.356121	1635.772545	16.309223
27.344952	1640.741499	16.314240
27.690144	1647.626691	16.319258
27.345062	1628.468301	16.324275
27.555432	1614.082239	16.329293
27.253594	1612.986677	16.334311
27.323627	1608.174658	16.339328
27.374235	1610.780177	16.344346
27.001093	1624.089686	16.349363
27.314865	1629.292303	16.354381
27.322502	1649.791856	16.359399
27.410808	1640.739785	16.364416
27.169922	1646.669410	16.369434
27.075006	1636.084249	16.374451
27.236498	1633.863249	16.379469
27.472030	1653.132396	16.384487
27.694807	1660.780833	16.389504
28.119307	1655.334318	16.394522
27.405573	1672.499834	16.399539
28.138469	1669.546105	16.404557
27.908260	1665.198194	16.409575
27.716408	1672.919090	16.414592
28.051421	1664.123048	16.419610
27.757150	1670.224081	16.424627
28.095158	1664.548384	16.429645
27.762737	1664.807099	16.434663
27.962234	1663.226184	16.439680
28.121569	1668.743075	16.444698
28.006641	1656.735218	16.449715
28.363955	1661.206536	16.454733
28.078405	1659.038541	16.459751
28.025636	1661.956584	16.464768
28.049546	1654.130731	16.469786
27.721707	1666.748828	16.474803
28.224049	1668.256422	16.479821
28.207073	1662.402804	16.484839
27.907781	1660.639191	16.489856
28.066873	1654.241000	16.494874
28.302372	1664.468680	16.499891
28.326833	1669.844888	16.504909
28.158881	1666.396606	16.509927
28.214461	1659.874789	16.514944
28.264522	1663.630448	16.519962
28.309500	1670.619781	16.524979
28.189401	1659.428021	16.529997
28.177021	1686.807758	16.535015
28.230219	1683.736258	16.540032
28.443813	1688.232908	16.545050
28.157444	1697.674128	16.550067
28.271572	1695.917185	16.555085
28.255133	1699.619087	16.560103
28.075764	1704.854014	16.565120
28.514670	1699.434430	16.570138
28.668750	1718.655513	16.575155
28.728994	1717.829200	16.580173
29.122014	1722.597746	16.585191
28.949808	1717.617876	16.590208
28.850486	1699.988264	16.595226
28.781715	1710.082617	16.600243
28.842261	1703.215321	16.605261
29.025045	1702.394740	16.610279
28.874412	1690.729327	16.615296
28.986219	1683.238297	16.620314
29.157476	1695.894006	16.625331
29.127311	1689.446377	16.630349
28.829678	1684.848220	16.635367
28.452683	1695.375925	16.640384
29.237693	1712.844536	16.645402
29.130084	1711.598972	16.650419
29.344133	1718.759181	16.655437
29.253635	1722.053697	16.660455
29.167085	1718.570891	16.665472
29.262140	1711.419186	16.670490
29.100210	1718.942863	16.675507
29.364281	1716.827718	16.680525
29.547516	1719.949260	16.685543
29.531162	1717.300413	16.690560
29.650240	1722.401788	16.695578
29.390864	1726.990187	16.700595
29.543653	1710.045186	16.705613
29.451243	1702.361151	16.710631
29.144800	1713.980608	16.715648
29.795931	1703.485673	16.720666
29.533241	1716.444771	16.725683
29.223259	1724.174387	16.730701
29.596037	1713.674662	16.735719
29.028441	1721.242150	16.740736
29.403300	1711.735455	16.745754
29.279185	1724.652569	16.750771
29.323302	1714.922217	16.755789
29.525912	1732.395567	16.760807
29.263835	1737.089716	16.765824
29.758938	1736.014401	16.770842
29.264878	1752.115294	16.775859
29.469284	1743.577965	16.780877
29.823704	1747.336099	16.785895
29.651325	1752.027634	16.790912
29.861211	1740.611229	16.795930
30.108779	1742.765774	16.800947
29.989029	1741.091758	16.805965
30.117650	1751.833549	16.810983
30.062309	1753.702170	16.816000
30.126536	1749.553580	16.821018
30.319751	1765.949132	16.826035
30.066433	1759.603105	16.831053
30.056140	1750.960126	16.836071
30.299958	1771.399358	16.841088
30.495594	1765.624135	16.846106
30.427190	1763.038205	16.851123
30.429653	1747.671151	16.856141
30.171701	1738.774653	16.861159
29.952608	1752.832536	16.866176
30.594666	1756.568531	16.871194
30.531266	1769.210722	16.876211
30.538119	1773.033974	16.881229
30.320480	1771.010233	16.886247
30.289620	1768.805647	16.891264
30.818409	1769.335187	16.896282
30.772667	1772.451276	16.901299
30.702266	1772.892059	16.906317
30.258855	1770.949519	16.911335
30.392641	1767.483828	16.916352
30.634678	1763.345019	16.921370
30.451278	1770.856917	16.926387
30.457104	1766.664042	16.931405
30.559031	1764.733145	16.936423
30.296635	1776.925611	16.941440
30.778156	1773.304635	16.946458
30.622158	1777.581122	16.951475
30.688286	1784.111164	16.956493
31.019155	1799.469567	16.961511
30.822196	1807.584435	16.966528
31.439321	1793.750007	16.971546
31.216722	1800.357488	16.976563
31.197945	1788.299195	16.981581
31.113493	1768.714736	16.986599
30.821952	1764.131097	16.991616
31.152090	1773.577955	16.996634
31.255431	1776.045277	17.001651
31.432887	1789.522178	17.006669
31.021464	1765.748592	17.011687
30.781036	1788.203445	17.016704
31.182474	1795.219943	17.021722
31.073643	1794.069051	17.026739
31.238351	1789.854049	17.031757
31.355069	1794.065399	17.036775
31.406780	1794.842848	17.041792
31.339334	1799.419629	17.046810
31.588739	1801.505777	17.051827
31.753582	1794.694031	17.056845
31.639529	1795.872448	17.061863
31.231595	1809.561834	17.066880
31.637361	1791.357967	17.071898
31.647069	1793.406764	17.076915
31.433223	1802.702617	17.081933
31.602704	1795.561209	17.086951
31.595554	1801.617996	17.091968
31.446608	1793.293931	17.096986
31.611260	1807.030215	17.102003
32.115138	1808.621220	17.107021
32.310101	1800.837883	17.112039
31.098455	1796.509416	17.117056
31.580089	1793.518258	17.122074
32.071163	1808.447492	17.127091
31.850142	1818.243887	17.132109
31.829990	1809.545621	17.137127
32.084851	1820.115831	17.142144
32.055962	1810.458499	17.147162
32.201346	1810.638063	17.152179
32.095088	1822.018641	17.157197
32.467897	1810.683713	17.162215
32.137889	1816.844441	17.167232
32.267712	1809.655059	17.172250
31.982645	1810.891851	17.177267
32.206444	1819.714854	17.182285
32.131116	1824.589168	17.187303
31.892894	1816.102306	17.192320
32.094211	1815.759896	17.197338
32.095608	1816.841293	17.202355
32.179927	1830.106484	17.207373
32.684631	1842.092919	17.212391
32.547812	1845.860216	17.217408
32.849124	1842.839405	17.222426
33.074954	1846.512724	17.227443
32.322952	1829.109307	17.232461
32.566879	1812.539046	17.237479
32.370557	1816.338212	17.242496
32.553541	1830.692473	17.247514
32.733021	1839.031140	17.252531
32.767787	1839.163834	17.257549
32.781598	1836.909933	17.262567
32.739524	1839.253084	17.267584
32.831243	1840.667152	17.272602
33.115676	1845.196232	17.277619
32.822785	1845.524785	17.282637
32.944332	1834.445900	17.287655
32.859267	1845.458866	17.292672
32.769594	1843.353346	17.297690
32.887755	1835.011888	17.302707
32.826356	1837.763301	17.307725
33.037831	1841.491937	17.312743
32.721273	1841.151453	17.317760
32.879258	1831.171728	17.322778
32.908149	1838.292126	17.327795
32.748316	1847.260025	17.332813
33.279747	1854.007462	17.337831
33.047988	1869.065452	17.342848
33.293553	1873.303754	17.347866
33.363102	1869.068830	17.352883
33.221338	1869.162790	17.357901
33.578219	1870.798957	17.362919
33.387405	1862.420953	17.367936
33.301947	1867.487876	17.372954
33.757705	1856.335246	17.377971
33.287509	1862.263875	17.382989
33.469204	1870.756701	17.388007
33.483531	1861.341181	17.393024
33.649670	1865.328859	17.398042
33.681310	1856.319880	17.403059
33.537942	1868.733074	17.408077
33.625092	1854.579132	17.413095
33.806140	1863.893418	17.418112
33.710912	1893.016331	17.423130
34.095078	1892.393931	17.428147
34.148625	1881.617946	17.433165
34.324412	1868.118162	17.438183
34.216196	1870.020531	17.443200
34.070426	1860.230925	17.448218
34.064374	1862.390984	17.453235
33.893660	1862.798352	17.458253
33.906973	1864.490307	17.463271
33.888278	1867.141963	17.468288
33.901183	1871.524998	17.473306
34.021503	1877.141904	17.478323
33.831034	1899.187136	17.483341
34.216197	1896.736444	17.488359
33.958065	1902.620400	17.493376
34.015484	1904.002352	17.498394
34.079213	1891.836654	17.503411
33.912294	1895.586695	17.508429
34.346997	1910.755041	17.513447
34.326327	1906.669447	17.518464
34.604088	1906.316766	17.523482
34.931732	1902.963678	17.528499
34.706670	1912.816306	17.533517
34.851320	1891.141518	17.538535
34.716524	1885.461991	17.543552
34.746537	1862.965539	17.548570
34.877063	1877.048034	17.553587
34.709469	1878.469725	17.558605
35.030114	1873.120601	17.563623
35.291813	1869.986857	17.568640
35.173457	1868.748568	17.573658
34.978610	1874.614970	17.578675
34.890462	1885.032876	17.583693
35.380817	1885.274713	17.588711
35.249612	1882.766061	17.593728
35.132317	1882.792010	17.598746
35.441541	1868.586595	17.603763
34.892340	1860.057014	17.608781
34.907855	1860.964843	17.613799
35.190090	1877.762289	17.618816
34.905018	1883.147207	17.623834
35.037902	1883.765990	17.628851
34.930259	1886.235324	17.633869
34.813012	1880.125785	17.638887
34.928841	1889.837037	17.643904
35.132791	1884.073781	17.648922
35.169554	1884.531304	17.653939
35.144955	1891.661746	17.658957
35.566245	1902.113577	17.663975
35.541828	1902.427881	17.668992
35.460420	1902.953351	17.674010
35.738060	1911.240014	17.679027
35.372155	1907.654920	17.684045
35.827633	1906.187174	17.689063
35.604902	1905.169058	17.694080
35.598028	1903.149639	17.699098
35.653336	1909.168001	17.704115
35.535458	1907.522985	17.709133
35.910796	1900.024519	17.714151
35.645370	1903.396989	17.719168
35.499904	1908.459276	17.724186
35.739594	1901.984483	17.729203
35.449792	1905.441090	17.734221
35.479833	1908.746826	17.739239
35.590232	1908.020273	17.744256
35.513266	1929.570865	17.749274
35.992502	1931.668259	17.754291
35.757063	1945.117081	17.759309
36.226234	1929.285565	17.764327
35.805021	1935.641311	17.769344
35.825233	1939.321271	17.774362
35.937462	1928.965034	17.779379
36.180856	1947.188099	17.784397
36.388076	1954.657778	17.789415
36.572130	1966.441028	17.794432
36.643681	1956.621354	17.799450
37.170747	1948.307333	17.804467
36.717109	1942.372437	17.809485
37.077329	1930.665332	17.814503
36.923005	1925.697595	17.819520
36.796474	1927.431955	17.824538
37.038289	1912.954011	17.829555
37.079743	1919.704304	17.834573
36.913256	1916.734800	17.839591
37.125996	1897.656513	17.844608
36.778493	1890.591043	17.849626
36.715313	1885.670258	17.854643
36.578214	1880.127317	17.859661
37.174092	1880.651287	17.864679
36.789772	1885.659740	17.869696
36.689830	1887.945344	17.874714
36.973780	1885.718243	17.879731
36.859764	1911.879104	17.884749
36.907674	1918.579320	17.889767
37.142630	1917.205290	17.894784
37.067033	1926.631700	17.899802
37.009257	1914.958251	17.904819
36.722183	1916.194398	17.909837
36.750986	1916.270605	17.914855
37.095746	1909.003932	17.919872
36.780803	1904.767974	17.924890
37.273119	1905.874542	17.929907
36.933083	1920.675901	17.934925
37.031166	1948.503149	17.939943
37.297109	1943.410649	17.944960
37.150408	1955.126907	17.949978
37.507658	1935.159637	17.954995
37.154492	1940.182052	17.960013
37.330116	1961.868882	17.965031
37.377062	1950.567033	17.970048
37.086967	1943.776074	17.975066
37.245354	1961.747880	17.980083
37.266603	1977.895533	17.985101
37.561140	1973.667884	17.990119
37.655568	1985.657669	17.995136
37.460246	1981.869980	18.000154
37.772302	1973.589703	18.005171
37.811756	1994.377336	18.010189
37.898697	1975.278407	18.015207
37.953752	1977.532309	18.020224
38.131811	1986.598373	18.025242
38.135814	1981.977444	18.030259
37.841558	1972.396731	18.035277
38.082614	1992.570406	18.040295
38.475945	2002.484073	18.045312
38.043460	2003.737367	18.050330
38.252346	2005.177163	18.055347
38.336246	2007.116692	18.060365
38.318462	2010.780313	18.065383
38.421007	1996.434741	18.070400
38.418286	2012.689529	18.075418
38.645064	2005.845215	18.080435
38.720419	2008.928154	18.085453
38.524967	2006.292122	18.090471
38.685981	2007.683732	18.095488
39.061606	1997.527204	18.100506
38.620856	1985.139319	18.105523
38.679640	1980.468003	18.110541
38.769706	1968.757880	18.115559
38.900014	1962.756202	18.120576
38.573863	1968.797469	18.125594
38.879596	1975.206118	18.130611
38.757878	1973.633769	18.135629
38.863617	1980.290404	18.140647
38.758253	2001.796780	18.145664
38.884801	1996.386392	18.150682
39.066298	1992.108922	18.155699
39.135506	1994.934241	18.160717
39.174259	2007.372170	18.165735
39.209596	1992.285431	18.170752
38.999099	2005.425494	18.175770
39.181713	2009.025688	18.180787
39.105745	2001.305917	18.185805
38.926689	1997.755075	18.190823
39.161921	2001.870726	18.195840
39.115438	1999.885199	18.200858
39.165941	1997.551597	18.205875
39.226349	2007.011088	18.210893
39.230565	2005.417137	18.215911
39.414326	2001.697495	18.220928
39.181305	2026.152818	18.225946
39.439084	2031.361282	18.230963
39.634789	2035.706284	18.235981
39.447377	2036.041817	18.240999
39.445496	2039.538268	18.246016
39.191055	2041.413252	18.251034
39.524445	2032.238769	18.256051
39.591074	2027.486428	18.261069
39.407327	2037.902519	18.266087
39.758000	2049.282751	18.271104
39.660997	2063.702588	18.276122
40.060117	2067.722678	18.281139
39.967773	2063.756749	18.286157
39.949448	2062.975878	18.291175
40.384388	2065.366406	18.296192
40.116412	2066.050846	18.301210
40.492111	2067.911853	18.306227
40.202306	2067.532891	18.311245
40.051830	2061.036294	18.316263
40.020003	2063.006173	18.321280
40.003324	2067.069187	18.326298
39.898251	2066.278244	18.331315
40.040600	2063.091751	18.336333
40.004255	2061.218898	18.341351
40.350794	2066.580799	18.346368
40.137387	2085.724302	18.351386
40.271955	2083.319125	18.356403
40.717766	2095.241286	18.361421
40.366459	2104.298055	18.366439
40.308713	2094.330780	18.371456
40.589002	2088.727453	18.376474
40.608335	2092.145418	18.381491
40.865511	2092.528733	18.386509
41.003507	2083.016469	18.391527
41.023973	2088.386398	18.396544
40.598938	2099.877922	18.401562
41.007977	2083.288550	18.406579
41.204302	2075.210788	18.411597
41.165378	2089.369111	18.416615
41.236908	2092.824313	18.421632
40.960921	2093.521494	18.426650
41.143115	2078.459217	18.431667
41.279074	2082.402534	18.436685
41.006283	2084.957255	18.441703
41.186911	2072.587472	18.446720
41.410654	2097.465211	18.451738
41.627682	2107.313011	18.456755
41.233489	2088.981760	18.461773
41.226917	2089.854280	18.466791
41.784094	2104.373907	18.471808
41.562983	2098.335572	18.476826
41.713245	2101.027648	18.481843
41.636916	2104.860791	18.486861
41.559275	2099.673261	18.491879
41.768383	2101.261439	18.496896
41.488338	2101.087337	18.501914
41.438901	2108.520968	18.506931
41.774587	2108.158907	18.511949
41.473083	2106.040723	18.516967
41.627277	2110.592191	18.521984
41.688225	2110.300133	18.527002
41.575004	2103.189552	18.532019
42.007436	2114.649816	18.537037
42.078461	2128.921882	18.542055
42.084203	2124.377583	18.547072
42.143805	2130.114446	18.552090
42.046630	2139.687253	18.557107
42.275981	2141.394715	18.562125
42.485362	2126.618420	18.567143
42.544533	2125.032106	18.572160
42.409350	2131.892775	18.577178
42.132803	2127.373274	18.582195
42.637262	2132.438658	18.587213
42.231743	2129.987695	18.592231
42.296542	2130.082362	18.597248
42.367146	2137.973877	18.602266
42.169120	2117.854847	18.607283
42.452481	2131.211409	18.612301
42.372117	2129.351136	18.617319
42.428917	2125.773691	18.622336
42.236999	2129.740890	18.627354
42.700277	2140.730376	18.632371
42.560612	2145.129843	18.637389
42.486023	2159.246687	18.642407
42.735187	2164.435363	18.647424
42.970245	2159.250662	18.652442
42.749575	2162.433331	18.657459
42.554330	2160.114529	18.662477
42.534809	2160.986830	18.667495
42.738059	2190.117275	18.672512
43.238828	2188.971711	18.677530
43.471593	2182.477278	18.682547
43.769284	2193.267219	18.687565
43.637030	2185.637947	18.692583
43.697746	2156.825019	18.697600
43.906081	2143.317254	18.702618
43.716207	2138.443305	18.707635
44.191644	2133.887720	18.712653
43.814262	2148.301020	18.717671
43.942596	2131.097815	18.722688
44.117169	2141.786030	18.727706
43.414400	2135.535964	18.732723
43.963975	2115.641591	18.737741
43.736621	2119.697507	18.742759
43.838568	2119.662229	18.747776
43.959814	2122.131766	18.752794
43.603210	2125.164073	18.757811
43.778481	2119.957379	18.762829
43.667908	2137.227457	18.767847
44.199810	2136.134620	18.772864
43.850038	2130.091551	18.777882
43.502762	2133.828544	18.782899
43.966903	2124.850488	18.787917
43.794649	2130.289872	18.792935
43.720536	2136.345652	18.797952
44.198491	2148.713481	18.802970
44.304880	2163.324779	18.807987
44.489747	2164.956729	18.813005
44.071196	2167.248571	18.818023
43.988334	2167.258003	18.823040
43.989431	2171.028767	18.828058
44.002911	2166.566043	18.833075
44.334780	2167.048620	18.838093
44.322855	2180.499291	18.843111
44.229376	2176.653586	18.848128
44.769028	2197.640896	18.853146
44.385858	2194.023157	18.858163
44.762767	2174.601487	18.863181
44.696814	2188.234107	18.868199
44.886883	2200.649155	18.873216
44.843689	2189.850166	18.878234
44.653407	2187.027637	18.883251
44.575891	2196.804297	18.888269
44.980046	2211.397732	18.893287
45.171179	2218.373004	18.898304
45.457538	2214.591480	18.903322
45.249019	2215.151152	18.908339
45.070708	2187.968057	18.913357
45.098179	2214.152698	18.918375
45.112456	2219.171171	18.923392
45.242247	2218.745307	18.928410
45.184665	2217.781367	18.933427
45.697923	2212.719362	18.938445
45.045170	2224.320254	18.943463
45.152628	2220.563763	18.948480
45.340619	2216.505412	18.953498
45.204855	2220.255501	18.958515
45.121493	2219.267477	18.963533
45.402656	2231.015593	18.968551
45.997851	2235.651295	18.973568
46.206585	2244.993715	18.978586
45.770070	2244.346893	18.983603
46.083832	2237.492826	18.988621
46.157485	2257.517363	18.993639
45.852067	2230.367794	18.998656
46.042904	2216.734522	19.003674
45.945319	2240.966054	19.008691
45.943455	2233.428784	19.013709
46.214679	2244.444176	19.018727
45.928169	2246.396327	19.023744
46.363789	2240.920018	19.028762
46.014592	2239.742479	19.033779
46.466978	2234.069130	19.038797
46.146669	2234.107958	19.043815
46.312564	2240.558526	19.048832
46.475970	2236.263704	19.053850
46.379938	2235.487989	19.058867
46.621973	2230.747934	19.063885
46.642061	2231.108626	19.068903
46.889192	2232.208299	19.073920
46.736875	2230.406946	19.078938
46.339427	2235.013586	19.083955
46.650435	2228.505812	19.088973
46.501112	2250.564233	19.093991
46.586621	2263.472548	19.099008
46.937962	2265.249818	19.104026
46.626742	2265.235771	19.109043
47.164100	2263.230105	19.114061
46.769409	2274.187266	19.119079
46.860495	2264.926320	19.124096
47.380827	2271.168542	19.129114
47.194992	2277.717203	19.134131
47.176046	2261.603836	19.139149
47.410733	2268.796715	19.144167
47.296389	2279.014511	19.149184
47.276796	2268.188537	19.154202
47.278625	2267.500379	19.159219
47.281906	2267.482390	19.164237
47.018177	2290.590579	19.169255
47.453898	2296.133081	19.174272
47.915308	2297.053270	19.179290
48.005234	2301.834290	19.184307
48.160048	2304.019793	19.189325
47.775590	2294.842330	19.194343
48.090044	2289.498811	19.199360
47.838099	2287.572393	19.204378
47.826883	2294.683096	19.209395
48.035530	2286.134137	19.214413
47.870343	2288.357163	19.219431
47.936148	2292.515454	19.224448
48.133124	2288.408557	19.229466
48.275661	2290.051255	19.234483
48.282090	2295.156278	19.239501
48.380455	2283.004233	19.244519
48.204853	2282.819955	19.249536
48.431829	2277.129316	19.254554
48.200428	2278.214965	19.259571
48.312608	2285.173002	19.264589
48.170234	2295.424374	19.269607
47.992694	2274.087695	19.274624
48.142110	2280.143402	19.279642
48.311328	2300.866900	19.284659
48.423899	2304.519679	19.289677
48.422863	2321.573455	19.294695
48.710496	2321.771642	19.299712
48.803880	2312.062101	19.304730
48.528067	2301.150305	19.309747
48.901424	2308.501177	19.314765
48.986515	2304.337377	19.319783
48.300003	2310.915642	19.324800
49.037881	2300.868921	19.329818
49.120771	2307.857199	19.334835
48.968563	2305.887725	19.339853
48.927887	2321.900512	19.344871
48.974626	2343.460963	19.349888
49.079259	2338.562691	19.354906
49.207882	2346.612033	19.359923
49.114607	2341.814962	19.364941
49.297494	2337.840486	19.369959
49.361073	2341.383467	19.374976
49.210550	2335.424704	19.379994
49.089190	2349.570906	19.385011
49.791202	2354.945816	19.390029
49.981270	2360.831466	19.395047
49.794893	2374.097766	19.400064
49.915924	2367.329423	19.405082
49.995439	2361.084431	19.410099
49.953302	2342.938577	19.415117
50.080135	2343.490669	19.420135
49.781058	2342.936081	19.425152
50.014170	2342.469914	19.430170
50.013644	2362.260410	19.435187
50.312059	2348.519884	19.440205
50.283225	2349.620683	19.445223
50.500318	2360.824418	19.450240
51.021325	2341.971981	19.455258
50.320781	2332.308390	19.460275
50.562506	2322.781003	19.465293
50.418227	2309.273885	19.470311
50.259833	2316.356364	19.475328
50.310812	2316.816471	19.480346
50.732581	2330.428263	19.485363
50.813611	2329.068610	19.490381
50.667170	2336.546134	19.495399
50.423518	2349.328615	19.500416
50.599543	2340.596058	19.505434
50.268288	2355.294028	19.510451
50.505915	2351.339044	19.515469
50.961639	2348.603026	19.520487
50.891827	2352.445782	19.525504
50.833014	2338.505656	19.530522
51.037735	2345.004177	19.535539
50.526998	2348.950695	19.540557
50.899184	2363.188961	19.545575
50.716062	2376.627741	19.550592
51.107345	2372.939067	19.555610
50.951249	2380.525678	19.560627
51.241790	2376.006874	19.565645
51.396031	2367.098981	19.570663
51.140421	2389.542650	19.575680
51.535377	2400.072395	19.580698
51.647600	2410.479000	19.585715
51.617752	2408.010398	19.590733
51.883601	2405.646661	19.595751
51.635044	2408.629675	19.600768
51.739654	2407.597193	19.605786
51.840908	2413.245593	19.610803
51.609453	2421.903443	19.615821
51.701607	2402.095509	19.620839
51.371441	2414.501035	19.625856
51.862548	2409.209380	19.630874
51.693091	2418.852961	19.635891
51.628693	2421.511674	19.640909
52.355454	2430.245028	19.645927
52.514285	2437.357812	19.650944
52.974988	2439.050502	19.655962
52.839047	2423.117309	19.660979
52.421089	2409.004990	19.665997
52.279809	2404.511475	19.671015
52.670781	2402.096357	19.676032
52.529857	2397.383317	19.681050
52.973130	2403.469641	19.686067
52.647141	2403.003152	19.691085
52.814395	2397.194200	19.696103
52.285771	2385.958206	19.701120
52.822911	2381.436248	19.706138
52.614354	2390.016878	19.711155
52.653212	2399.429978	19.716173
52.733739	2403.142008	19.721191
52.872444	2421.924030	19.726208
52.844376	2432.392608	19.731226
53.190329	2414.276036	19.736243
53.066506	2416.833357	19.741261
53.322116	2419.937178	19.746279
53.020613	2416.668655	19.751296
52.948485	2418.117529	19.756314
53.454250	2428.591387	19.761331
53.514751	2407.446074	19.766349
53.528562	2403.439683	19.771367
53.084459	2423.194904	19.776384
53.378327	2432.623755	19.781402
53.674022	2446.305100	19.786419
53.683349	2444.465989	19.791437
53.814841	2444.186085	19.796455
54.041931	2449.821381	19.801472
53.910944	2447.917274	19.806490
53.960943	2444.918784	19.811507
53.871399	2439.889195	19.816525
54.025710	2441.567559	19.821543
53.733420	2440.292025	19.826560
53.823531	2437.459728	19.831578
54.235779	2439.827691	19.836595
54.005874	2440.707413	19.841613
53.958686	2435.316329	19.846631
53.718929	2454.953578	19.851648
54.144728	2458.803236	19.856666
54.472721	2470.294606	19.861683
54.110025	2473.749605	19.866701
54.581708	2466.630780	19.871719
54.664383	2465.174198	19.876736
54.558680	2467.876158	19.881754
54.750608	2474.461881	19.886771
54.758690	2479.933000	19.891789
54.654375	2468.566798	19.896807
54.603169	2475.484995	19.901824
54.843457	2486.172433	19.906842
55.029226	2496.664967	19.911859
55.387301	2502.145774	19.916877
55.294879	2481.374421	19.921895
55.263391	2478.678145	19.926912
55.150266	2461.037542	19.931930
55.577906	2461.306486	19.936947
55.147270	2473.411168	19.941965
55.279360	2475.416804	19.946983
55.554673	2490.949240	19.952000
55.589817	2498.653114	19.957018
55.525924	2500.862778	19.962035
55.792394	2491.187312	19.967053
55.790749	2493.527819	19.972071
55.524608	2474.645266	19.977088
55.687698	2482.806297	19.982106
55.685830	2489.315200	19.987123
55.286040	2489.143360	19.992141
56.084056	2484.384973	19.997159
55.741678	2485.129358	20.002176
55.814333	2487.529037	20.007194
56.012981	2495.740297	20.012211
55.972866	2496.860883	20.017229
56.132662	2489.595175	20.022247
56.009062	2487.344004	20.027264
55.942875	2493.350587	20.032282
55.893026	2498.212439	20.037299
56.060097	2514.063941	20.042317
56.184876	2516.298724	20.047335
56.210323	2531.994528	20.052352
56.380886	2530.111639	20.057370
56.252811	2519.006588	20.062387
56.546399	2522.806462	20.067405
56.989231	2532.289296	20.072423
56.764952	2535.807256	20.077440
56.840800	2556.661477	20.082458
57.093001	2545.156391	20.087475
56.662641	2557.474659	20.092493
57.186262	2559.578981	20.097511
56.941931	2562.686119	20.102528
56.786447	2560.244946	20.107546
57.154774	2552.592022	20.112563
56.967578	2548.102903	20.117581
56.906677	2545.301051	20.122599
56.957887	2541.585468	20.127616
57.051937	2550.335851	20.132634
57.321577	2552.133349	20.137651
57.671227	2567.515006	20.142669
57.584134	2572.329890	20.147687
57.894503	2573.362056	20.152704
57.489846	2568.431539	20.157722
57.690927	2564.503208	20.162739
57.761791	2572.647836	20.167757
57.727768	2560.072404	20.172775
57.923773	2562.878844	20.177792
57.848703	2566.546552	20.182810
57.939885	2552.522790	20.187827
57.760141	2568.650144	20.192845
57.968229	2569.102013	20.197863
58.186657	2578.457599	20.202880
58.130870	2587.050689	20.207898
58.318085	2590.093609	20.212915
57.894880	2604.490891	20.217933
58.387302	2588.778079	20.222951
58.496590	2590.396582	20.227968
58.254514	2596.946011	20.232986
58.666827	2587.583762	20.238003
58.195957	2600.331364	20.243021
58.273670	2603.683895	20.248039
58.522839	2601.721084	20.253056
58.442942	2617.648539	20.258074
58.861226	2618.544972	20.263091
58.620637	2623.479323	20.268109
58.750675	2626.523037	20.273127
59.281385	2608.961886	20.278144
58.969002	2610.036532	20.283162
59.321742	2631.272234	20.288179
59.328491	2640.996867	20.293197
59.630553	2629.412028	20.298215
59.378199	2619.943269	20.303232
59.554223	2618.565729	20.308250
59.781141	2600.063325	20.313267
59.234565	2610.569085	20.318285
59.594513	2599.185908	20.323303
59.460178	2613.357328	20.328320
59.289749	2642.170679	20.333338
59.875812	2637.744296	20.338355
59.597772	2627.626477	20.343373
60.082476	2635.899788	20.348391
59.864599	2635.295356	20.353408
60.042316	2637.735173	20.358426
60.691930	2633.227036	20.363443
60.359063	2645.391674	20.368461
60.348924	2633.640917	20.373479
60.478848	2638.135926	20.378496
60.394712	2637.192488	20.383514
60.630662	2630.374727	20.388531
60.635169	2641.103989	20.393549
60.446990	2634.749000	20.398567
60.429425	2638.397774	20.403584
60.390883	2636.655520	20.408602
60.357701	2633.014879	20.413619
60.445424	2628.700765	20.418637
60.634161	2632.631172	20.423655
60.797705	2632.456198	20.428672
60.610536	2633.344418	20.433690
60.545632	2633.573899	20.438707
60.470472	2653.171603	20.443725
60.824937	2663.022638	20.448743
60.844494	2657.172251	20.453760
60.697641	2663.186324	20.458778
61.043726	2661.644271	20.463795
61.128622	2688.256417	20.468813
61.068836	2682.964566	20.473831
61.267617	2690.026578	20.478848
61.342684	2686.701676	20.483866
61.458386	2688.337239	20.488883
61.381886	2695.445528	20.493901
61.387594	2693.985700	20.498919
61.460992	2694.784020	20.503936
61.378953	2717.465607	20.508954
61.590999	2720.383591	20.513971
61.460391	2723.162541	20.518989
61.711591	2717.171104	20.524007
61.643264	2726.255879	20.529024
61.757621	2743.171572	20.534042
62.585431	2741.979016	20.539059
62.546767	2739.782666	20.544077
62.964825	2738.165726	20.549095
62.869158	2715.761629	20.554112
62.744341	2708.487735	20.559130
63.065931	2705.775002	20.564147
62.983583	2700.684300	20.569165
63.164963	2706.035532	20.574183
63.031521	2707.520546	20.579200
63.026243	2699.252559	20.584218
62.930520	2699.271400	20.589235
62.965071	2693.995253	20.594253
63.017153	2686.886613	20.599271
63.263277	2701.194248	20.604288
62.995469	2702.366841	20.609306
63.496280	2696.463095	20.614323
63.026242	2695.166126	20.619341
62.865996	2693.389649	20.624359
63.365093	2696.782208	20.629376
62.971984	2699.064409	20.634394
63.365520	2690.089428	20.639411
63.559209	2702.796587	20.644429
63.533583	2696.481833	20.649447
63.662450	2693.808034	20.654464
63.028845	2686.505042	20.659482
63.374570	2704.500298	20.664499
63.490042	2711.911496	20.669517
63.639791	2714.771275	20.674535
63.938712	2727.262850	20.679552
63.609388	2742.028579	20.684570
63.976803	2731.629243	20.689587
63.961876	2734.311132	20.694605
63.761525	2729.959951	20.699623
63.847696	2733.264856	20.704640
63.808056	2744.992168	20.709658
63.942897	2745.870686	20.714675
63.758421	2758.469328	20.719693
63.570213	2767.629444	20.724711
64.460143	2770.767292	20.729728
64.403575	2785.008887	20.734746
64.592407	2785.293090	20.739763
64.647716	2789.090477	20.744781
64.708703	2796.569771	20.749799
64.801221	2791.216694	20.754816
64.486180	2787.528897	20.759834
64.623250	2781.042154	20.764851
64.954396	2797.680564	20.769869
64.782422	2818.138518	20.774887
65.310106	2810.774274	20.779904
65.483962	2816.518889	20.784922
65.294189	2803.477096	20.789939
64.982281	2815.621673	20.794957
65.501011	2812.730291	20.799975
65.412446	2802.060607	20.804992
65.624448	2802.180361	20.810010
65.600066	2807.540433	20.815027
65.616806	2808.671527	20.820045
65.461114	2809.564201	20.825063
65.496901	2824.592491	20.830080
65.641112	2841.909831	20.835098
65.700867	2840.088323	20.840115
65.776766	2848.110421	20.845133
66.012146	2838.017855	20.850151
66.027012	2831.137923	20.855168
65.925517	2842.451343	20.860186
66.211716	2856.993037	20.865203
66.264725	2871.615795	20.870221
66.232198	2880.862451	20.875239
66.520380	2867.989249	20.880256
66.675634	2867.140878	20.885274
66.547913	2862.985520	20.890291
66.573951	2870.130092	20.895309
66.333988	2853.996727	20.900327
66.605679	2857.813884	20.905344
66.893275	2884.919616	20.910362
66.945712	2872.647538	20.915379
66.944221	2892.465642	20.920397
66.716886	2899.477303	20.925415
67.385003	2883.407228	20.930432
67.459695	2891.501591	20.935450
67.464676	2892.420473	20.940467
67.449241	2881.033571	20.945485
67.643885	2889.428567	20.950503
67.551300	2893.303565	20.955520
67.741849	2879.025699	20.960538
67.890304	2895.339699	20.965555
67.852855	2892.258727	20.970573
67.503471	2893.051135	20.975591
67.685152	2883.753590	20.980608
67.518515	2892.611413	20.985626
68.008200	2877.897132	20.990643
68.124146	2871.830747	20.995661
67.862982	2888.133689	21.000679
68.378788	2883.942457	21.005696
68.034955	2876.961943	21.010714
68.032754	2896.419167	21.015731
68.003756	2888.670128	21.020749
68.454474	2901.887113	21.025767
68.635187	2904.906762	21.030784
68.508163	2922.828037	21.035802
68.665413	2907.470273	21.040819
68.810945	2911.143339	21.045837
68.546090	2908.466849	21.050855
68.625345	2903.586766	21.055872
68.419876	2910.490887	21.060890
68.426268	2913.897591	21.065907
68.739743	2917.433858	21.070925
68.528187	2940.420819	21.075943
68.617474	2947.306170	21.080960
68.790222	2935.589330	21.085978
69.323505	2939.703028	21.090995
69.035632	2945.256679	21.096013
69.149343	2963.000827	21.101031
69.284778	2959.634987	21.106048
69.394465	2969.595167	21.111066
69.506333	2966.996174	21.116083
69.809828	2952.629896	21.121101
69.598637	2973.945672	21.126119
69.753443	2952.560224	21.131136
69.768829	2973.611407	21.136154
70.165224	2987.611813	21.141171
70.224461	2990.725564	21.146189
70.298092	2985.114924	21.151207
70.464185	2988.749180	21.156224
70.413317	2994.351083	21.161242
70.571963	2992.197090	21.166259
70.504844	2984.449578	21.171277
70.226756	2991.288572	21.176295
70.600757	2981.144663	21.181312
70.505534	2987.099544	21.186330
70.620163	2979.679465	21.191347
70.595142	2987.284081	21.196365
70.496799	2994.296910	21.201383
70.723547	2987.241352	21.206400
70.697086	2992.240825	21.211418
70.651029	3011.455453	21.216435
70.890018	3017.446061	21.221453
70.508478	3013.021201	21.226471
71.192328	3023.075114	21.231488
71.163205	3027.321925	21.236506
71.095579	3014.118044	21.241523
71.356951	3030.072598	21.246541
71.145618	3048.887830	21.251559
71.496937	3045.671330	21.256576
71.739082	3044.807017	21.261594
71.663767	3045.327383	21.266611
72.126837	3041.757788	21.271629
72.217753	3038.838244	21.276647
72.646647	3038.070626	21.281664
72.167629	3033.108350	21.286682
72.081751	3034.476879	21.291699
72.333664	3025.355824	21.296717
72.586615	3031.573648	21.301735
72.745791	3018.249613	21.306752
72.382425	3032.233878	21.311770
72.272179	3042.441854	21.316787
72.461310	3026.330313	21.321805
72.323202	3037.109793	21.326823
72.425617	3035.274914	21.331840
72.631203	3026.461106	21.336858
72.628946	3028.773252	21.341875
72.777997	3038.926176	21.346893
72.646133	3055.880732	21.351911
72.895112	3056.312081	21.356928
73.166368	3060.644693	21.361946
72.702276	3061.307251	21.366963
73.038670	3045.607557	21.371981
73.046923	3061.351225	21.376999
73.173141	3048.820764	21.382016
73.158243	3061.190458	21.387034
73.174720	3081.388102	21.392051
73.440543	3087.731768	21.397069
73.589557	3092.517247	21.402087
73.157052	3086.005207	21.407104
73.717430	3096.635453	21.412122
73.430946	3088.744223	21.417139
73.902999	3106.834030	21.422157
73.671035	3114.143390	21.427175
73.949734	3113.743486	21.432192
74.116896	3118.316533	21.437210
73.999642	3121.111457	21.442227
74.033160	3117.563219	21.447245
74.119032	3123.722078	21.452263
74.528316	3142.621873	21.457280
74.429971	3148.356474	21.462298
74.384683	3148.056560	21.467315
74.736108	3147.559995	21.472333
74.686140	3144.936535	21.477351
74.927397	3146.381328	21.482368
74.889886	3151.368900	21.487386
74.972697	3147.328277	21.492403
75.126218	3152.946069	21.497421
75.168515	3142.319878	21.502439
75.345637	3136.271627	21.507456
75.612941	3147.395987	21.512474
75.627782	3152.043031	21.517491
75.891218	3144.936460	21.522509
75.472126	3136.281715	21.527527
75.338559	3149.590344	21.532544
75.430077	3155.813634	21.537562
75.338299	3158.777969	21.542579
75.634202	3170.448387	21.547597
75.451154	3185.013206	21.552615
75.555189	3176.099957	21.557632
76.080058	3188.368750	21.562650
75.916096	3198.266819	21.567667
76.171257	3201.464769	21.572685
76.279253	3210.962408	21.577703
76.172165	3205.850038	21.582720
76.081182	3202.503056	21.587738
76.189647	3199.323112	21.592755
76.620325	3209.750072	21.597773
76.600693	3213.335939	21.602791
76.657349	3232.809843	21.607808
77.082511	3238.352072	21.612826
76.731349	3231.119072	21.617843
76.947532	3227.479605	21.622861
77.084989	3237.814490	21.627879
76.889633	3235.762658	21.632896
77.085072	3229.727879	21.637914
76.747612	3230.774623	21.642931
77.137311	3242.020948	21.647949
77.420806	3251.436071	21.652967
77.418324	3257.917840	21.657984
77.836347	3260.079081	21.663002
77.266187	3252.618487	21.668019
77.543650	3255.695445	21.673037
77.457065	3250.470620	21.678055
77.870148	3244.799465	21.683072
77.575804	3256.944634	21.688090
77.505216	3262.585324	21.693107
77.992597	3262.733199	21.698125
78.150097	3278.282746	21.703143
78.209962	3283.322377	21.708160
78.184417	3276.082401	21.713178
78.308358	3283.441689	21.718195
78.236658	3280.714713	21.723213
78.228502	3270.263696	21.728231
78.289370	3287.505152	21.733248
78.684035	3300.967563	21.738266
78.810571	3307.586297	21.743283
79.067514	3296.604069	21.748301
78.884262	3308.121096	21.753319
78.969174	3299.464078	21.758336
79.181819	3301.987598	21.763354
79.000283	3306.277779	21.768371
79.071367	3315.379624	21.773389
79.370308	3312.246527	21.778407
79.225089	3303.635013	21.783424
79.369694	3319.576485	21.788442
78.987902	3328.270114	21.793459
79.769280	3321.924311	21.798477
79.408168	3334.067187	21.803495
79.362758	3337.458922	21.808512
80.010529	3340.802651	21.813530
79.754733	3360.593298	21.818547
80.060787	3365.513538	21.823565
80.328013	3371.662607	21.828583
80.269482	3367.011834	21.833600
80.444518	3360.621329	21.838618
80.290743	3366.088012	21.843635
80.559240	3362.812694	21.848653
80.438895	3359.592575	21.853671
80.434131	3360.117435	21.858688
80.676616	3366.258385	21.863706
80.442360	3369.686844	21.868723
80.593003	3369.140775	21.873741
80.847521	3384.972422	21.878759
80.608833	3377.404241	21.883776
81.168180	3382.295231	21.888794
80.344180	3389.720657	21.893811
80.863470	3387.328675	21.898829
81.187597	3399.971351	21.903847
81.297998	3408.223466	21.908864
81.863981	3401.946294	21.913882
81.670866	3401.597181	21.918899
81.572355	3407.736227	21.923917
81.711238	3404.108705	21.928935
81.538887	3402.935707	21.933952
81.606090	3406.591126	21.938970
81.642869	3418.847844	21.943987
81.956155	3426.058592	21.949005
82.169383	3434.246881	21.954023
82.144072	3434.629078	21.959040
81.857645	3422.321223	21.964058
81.961713	3437.138042	21.969075
82.264627	3450.172052	21.974093
82.247851	3461.077836	21.979111
82.459232	3466.321227	21.984128
82.605880	3456.354732	21.989146
82.814509	3467.044144	21.994163
82.835907	3465.267483	21.999181
83.087027	3462.477685	22.004199
83.149261	3452.600729	22.009216
83.248265	3458.655978	22.014234
83.096233	3472.169505	22.019251
83.291481	3475.847876	22.024269
83.209242	3479.672492	22.029287
83.088072	3487.751107	22.034304
83.124802	3480.616097	22.039322
83.217879	3486.875877	22.044339
83.386943	3476.454491	22.049357
83.637781	3497.230081	22.054375
83.868206	3512.394197	22.059392
83.916947	3518.655016	22.064410
83.879845	3517.115178	22.069427
84.076667	3514.582370	22.074445
84.274804	3511.491086	22.079463
84.418351	3514.523689	22.084480
84.449351	3524.527149	22.089498
84.692551	3510.923065	22.094515
84.724898	3511.704786	22.099533
84.553312	3512.080448	22.104551
84.754931	3512.331844	22.109568
84.689774	3520.749247	22.114586
84.495401	3503.471860	22.119603
84.651273	3525.326943	22.124621
85.251327	3528.716393	22.129639
85.018081	3525.180254	22.134656
85.306271	3536.756555	22.139674
85.262258	3532.285614	22.144691
85.280731	3523.292998	22.149709
85.177981	3529.630427	22.154727
85.329819	3537.013966	22.159744
85.600487	3539.077550	22.164762
85.584755	3564.359029	22.169779
85.782216	3569.954357	22.174797
86.076646	3560.749193	22.179815
86.046051	3568.180214	22.184832
85.857620	3564.875240	22.189850
85.972497	3554.222602	22.194867
86.014349	3561.985739	22.199885
86.270760	3573.844874	22.204903
86.248541	3581.190266	22.209920
86.709677	3581.570434	22.214938
86.603245	3591.410034	22.219955
86.558278	3587.904579	22.224973
86.642711	3575.191624	22.229991
86.552933	3599.690129	22.235008
86.946554	3596.412985	22.240026
86.490551	3598.804130	22.245043
86.857876	3608.244202	22.250061
86.805676	3621.282310	22.255079
86.953568	3623.478004	22.260096
87.346552	3617.178939	22.265114
87.134871	3610.484519	22.270131
87.563388	3622.631393	22.275149
87.365518	3638.731751	22.280167
87.327700	3651.999397	22.285184
87.703127	3646.932347	22.290202
87.910636	3647.361118	22.295219
87.885895	3641.772796	22.300237
87.722769	3634.270742	22.305255
87.943691	3658.258161	22.310272
88.671799	3668.221721	22.315290
88.606079	3676.532608	22.320307
88.826831	3677.641866	22.325325
89.119155	3672.752319	22.330343
88.470210	3645.938913	22.335360
88.664134	3643.814829	22.340378
88.633718	3661.185956	22.345395
88.788814	3665.394233	22.350413
88.981725	3657.944360	22.355431
88.913438	3658.815158	22.360448
88.928274	3655.971455	22.365466
88.934236	3672.477535	22.370483
89.049583	3667.499910	22.375501
89.366241	3653.187110	22.380519
89.192685	3655.422538	22.385536
89.490068	3672.548964	22.390554
89.787047	3683.746366	22.395571
89.493125	3675.753308	22.400589
89.855934	3691.246116	22.405607
89.852028	3688.077554	22.410624
90.051948	3697.136681	22.415642
89.981159	3682.648506	22.420659
90.056764	3688.261257	22.425677
90.023018	3675.252789	22.430695
89.790840	3696.256490	22.435712
90.092649	3712.743254	22.440730
90.332903	3709.997727	22.445747
90.154939	3728.005907	22.450765
90.108800	3725.796282	22.455783
90.411497	3734.873094	22.460800
90.672562	3748.307577	22.465818
90.718477	3747.363841	22.470835
90.864507	3746.322065	22.475853
90.853726	3742.560140	22.480871
90.997191	3770.616435	22.485888
91.152974	3780.649835	22.490906
91.505865	3781.975455	22.495923
91.134244	3789.896004	22.500941
91.289412	3781.074353	22.505959
91.362140	3780.993114	22.510976
91.653174	3795.936863	22.515994
91.737917	3806.852099	22.521011
91.342790	3812.091101	22.526029
91.936034	3806.207691	22.531047
91.624394	3815.960081	22.536064
91.937656	3822.437157	22.541082
92.329820	3833.355158	22.546099
92.352485	3829.182958	22.551117
93.041656	3811.523011	22.556135
92.824350	3824.510619	22.561152
92.987391	3816.686864	22.566170
93.198393	3816.141044	22.571187
93.217107	3821.783322	22.576205
93.294955	3815.382313	22.581223
93.393781	3823.471994	22.586240
93.462426	3826.228058	22.591258
93.332300	3817.386992	22.596275
92.931765	3820.442235	22.601293
93.189085	3814.026531	22.606311
93.851504	3821.745525	22.611328
93.700408	3815.316204	22.616346
93.639718	3809.620768	22.621363
93.804256	3840.700492	22.626381
93.815238	3841.941274	22.631399
93.784957	3845.064477	22.636416
93.888121	3844.666396	22.641434
94.241002	3845.696747	22.646451
93.846965	3845.764683	22.651469
94.444680	3861.524755	22.656487
94.291989	3877.777738	22.661504
94.036213	3876.603133	22.666522
94.183623	3875.070566	22.671539
94.065314	3884.707588	22.676557
94.640797	3889.952771	22.681575
94.915999	3889.318780	22.686592
95.014712	3908.750756	22.691610
95.524853	3900.661729	22.696627
95.604375	3895.714755	22.701645
95.416068	3884.705291	22.706663
95.278412	3895.251823	22.711680
95.646893	3885.735017	22.716698
95.855017	3881.894759	22.721715
95.533051	3890.047313	22.726733
95.800667	3890.695690	22.731751
95.406386	3885.543541	22.736768
95.528822	3907.331065	22.741786
95.767498	3911.934658	22.746803
95.753683	3928.566325	22.751821
96.487203	3928.786534	22.756839
95.966543	3924.899757	22.761856
95.932822	3919.351008	22.766874
96.242081	3937.332072	22.771891
96.305078	3958.540899	22.776909
96.580090	3955.167531	22.781927
96.827729	3966.778414	22.786944
96.803857	3952.849959	22.791962
96.444790	3957.371230	22.796979
96.762511	3977.691919	22.801997
97.519355	3980.877609	22.807015
97.350807	3979.981894	22.812032
97.452689	3982.966356	22.817050
97.647763	3974.806121	22.822067
97.669374	3984.359454	22.827085
97.844472	3976.945444	22.832103
98.137812	3974.209603	22.837120
97.765960	3974.001428	22.842138
98.329993	3976.985904	22.847155
97.996518	3980.386795	22.852173
98.207210	3982.713897	22.857191
98.364250	3996.916583	22.862208
98.321971	4001.301662	22.867226
98.774278	3995.161938	22.872243
98.676403	4004.312186	22.877261
98.786046	3989.156499	22.882279
98.813737	3993.167804	22.887296
98.763446	3999.319588	22.892314
98.817353	3987.865691	22.897331
98.902563	4003.983825	22.902349
98.941106	4027.139338	22.907367
98.775155	4022.464385	22.912384
99.283518	4033.363327	22.917402
99.009778	4034.660621	22.922419
98.613476	4040.537699	22.927437
99.052184	4053.247805	22.932455
99.419090	4060.810628	22.937472
99.637294	4082.239258	22.942490
99.819752	4088.091983	22.947507
99.959797	4099.002224	22.952525
100.233484	4093.495927	22.957543
100.268502	4080.500955	22.962560
100.004621	4099.731660	22.967578
100.556112	4094.761362	22.972595
100.292953	4117.684178	22.977613
100.668572	4117.635175	22.982631
100.780911	4120.897469	22.987648
100.382553	4127.328870	22.992666
100.712797	4118.474949	22.997683
100.557356	4123.086640	23.002701
101.043127	4139.181247	23.007719
101.202039	4141.614570	23.012736
100.925804	4154.986609	23.017754
101.526404	4144.232835	23.022771
101.318108	4149.774550	23.027789
101.377767	4170.618460	23.032807
101.754271	4171.307914	23.037824
101.747668	4181.798338	23.042842
102.150476	4178.060883	23.047859
102.014462	4164.407863	23.052877
102.086265	4166.692193	23.057895
102.071788	4178.581985	23.062912
101.862945	4176.973999	23.067930
102.467467	4187.092574	23.072947
102.463899	4197.293917	23.077965
102.122595	4211.747259	23.082983
102.883298	4209.282195	23.088000
102.599622	4201.210004	23.093018
102.809475	4197.317021	23.098035
102.849462	4217.966208	23.103053
102.821421	4216.735442	23.108071
103.357307	4218.506075	23.113088
103.260184	4216.621350	23.118106
103.736371	4216.767153	23.123123
103.491213	4234.272044	23.128141
103.342981	4219.500093	23.133159
103.873743	4228.239896	23.138176
103.567728	4237.893978	23.143194
103.628704	4238.550923	23.148211
103.632409	4253.532354	23.153229
103.942579	4256.589935	23.158247
104.304500	4261.350439	23.163264
104.043394	4273.973205	23.168282
104.268464	4276.868861	23.173299
104.156396	4269.699020	23.178317
104.281714	4282.024075	23.183335
104.298969	4295.943428	23.188352
104.297279	4315.109421	23.193370
104.923238	4306.485282	23.198387
104.979251	4327.110705	23.203405
105.185366	4330.960720	23.208423
105.034206	4333.070885	23.213440
104.968355	4345.241744	23.218458
105.464824	4334.613712	23.223475
105.872371	4354.828317	23.228493
105.861383	4364.782560	23.233511
106.171711	4364.256926	23.238528
105.868265	4363.468127	23.243546
105.708849	4361.170038	23.248563
106.193650	4364.394069	23.253581
106.453974	4371.489990	23.258599
106.425714	4363.090067	23.263616
106.440171	4364.174799	23.268634
106.718023	4379.820923	23.273651
106.977385	4389.493100	23.278669
106.967940	4379.236046	23.283687
107.022115	4386.529823	23.288704
107.208638	4400.438625	23.293722
107.084991	4388.466899	23.298739
107.318022	4401.329785	23.303757
107.041797	4396.478837	23.308775
107.202515	4390.438718	23.313792
107.446742	4418.734268	23.318810
107.483751	4422.673668	23.323827
107.683139	4423.155776	23.328845
107.600790	4424.256114	23.333863
107.759996	4435.669353	23.338880
108.032317	4456.987191	23.343898
108.159078	4449.097064	23.348915
108.249912	4459.097538	23.353933
108.016675	4450.550720	23.358951
108.314667	4453.400895	23.363968
108.165566	4474.888002	23.368986
108.413478	4484.517640	23.374003
108.361199	4473.409294	23.379021
108.476530	4480.284723	23.384039
108.989752	4496.474384	23.389056
108.644910	4511.958951	23.394074
109.188111	4511.931867	23.399091
109.383017	4509.952000	23.404109
109.459572	4520.362767	23.409127
109.497107	4508.183598	23.414144
109.564977	4511.964765	23.419162
109.715715	4529.667182	23.424179
109.379824	4536.216780	23.429197
109.687384	4543.565618	23.434215
110.175860	4536.451154	23.439232
110.158303	4544.070260	23.444250
110.808547	4547.038635	23.449267
110.630747	4564.609147	23.454285
110.495506	4566.209993	23.459303
110.808915	4558.156286	23.464320
110.900728	4573.378597	23.469338
111.059031	4555.204319	23.474355
111.319292	4556.342155	23.479373
111.130165	4565.379456	23.484391
111.464960	4568.172781	23.489408
111.468331	4557.808369	23.494426
111.341696	4561.370886	23.499443
111.068519	4556.039438	23.504461
111.582080	4577.633345	23.509479
112.023740	4591.668279	23.514496
111.931729	4596.710991	23.519514
112.169348	4594.334270	23.524531
112.095643	4583.610115	23.529549
111.910995	4588.573244	23.534567
112.111886	4604.340190	23.539584
112.186945	4622.446183	23.544602
112.209073	4609.992300	23.549619
112.316908	4623.920997	23.554637
112.637007	4644.995751	23.559655
112.827449	4630.156032	23.564672
112.853191	4637.920399	23.569690
113.542840	4635.941449	23.574707
113.664667	4623.084839	23.579725
113.850774	4628.698964	23.584743
114.303761	4619.198854	23.589760
114.152941	4615.513797	23.594778
113.960297	4615.192136	23.599795
113.989719	4618.180424	23.604813
114.145803	4618.692923	23.609831
114.503925	4605.782322	23.614848
114.686270	4631.302505	23.619866
114.405425	4624.813573	23.624883
114.762813	4609.663594	23.629901
114.647778	4616.874016	23.634919
114.965806	4624.336130	23.639936
114.842732	4626.966919	23.644954
114.811019	4621.881787	23.649971
114.736219	4629.093834	23.654989
114.823878	4639.440243	23.660007
114.725672	4655.464155	23.665024
114.863291	4645.972042	23.670042
115.079772	4656.796418	23.675059
114.963086	4675.603093	23.680077
114.618471	4679.874136	23.685095
115.336737	4693.277596	23.690112
115.402289	4708.234283	23.695130
115.372534	4712.310387	23.700147
115.729295	4731.469635	23.705165
115.638366	4742.850410	23.710183
116.002308	4745.224752	23.715200
116.165396	4748.375637	23.720218
116.705340	4764.011914	23.725235
116.988637	4758.190784	23.730253
116.935401	4763.210999	23.735271
117.105178	4756.227055	23.740288
117.388117	4749.991394	23.745306
117.471744	4755.596511	23.750323
117.346668	4754.716403	23.755341
117.310908	4749.217698	23.760359
117.582841	4750.720180	23.765376
117.797899	4759.875071	23.770394
117.469612	4755.357831	23.775411
117.927046	4767.382315	23.780429
118.079588	4777.895667	23.785447
118.329525	4776.818150	23.790464
117.920420	4775.690858	23.795482
118.287584	4794.576794	23.800499
118.190422	4791.299785	23.805517
118.317698	4788.227047	23.810535
118.152393	4787.172076	23.815552
118.362139	4808.686969	23.820570
118.277847	4824.533152	23.825587
118.221915	4833.319449	23.830605
118.625155	4848.457891	23.835623
119.120438	4853.092599	23.840640
118.865712	4856.175131	23.845658
119.091316	4878.720250	23.850675
119.509526	4883.469678	23.855693
119.350615	4893.314439	23.860711
119.229109	4900.268954	23.865728
119.681024	4909.490317	23.870746
119.731977	4925.182355	23.875763
120.088989	4925.941214	23.880781
120.010006	4941.403144	23.885799
120.328595	4935.741485	23.890816
120.473591	4945.722691	23.895834
120.572762	4947.409656	23.900851
120.840683	4959.947923	23.905869
120.884342	4975.201026	23.910887
121.055241	4967.161995	23.915904
121.382137	4975.570918	23.920922
121.658900	4964.977977	23.925939
122.165157	4955.713370	23.930957
121.888726	4961.669023	23.935975
122.182503	4942.375368	23.940992
122.149661	4958.469111	23.946010
122.186674	4965.438411	23.951027
121.869476	4959.587285	23.956045
122.087632	4961.983781	23.961063
122.037647	4963.192991	23.966080
122.242646	4968.446609	23.971098
122.458472	4975.170996	23.976115
122.911797	4974.130732	23.981133
122.655861	4992.124904	23.986151
122.762654	4979.871714	23.991168
123.015156	4985.131663	23.996186
122.749054	5010.069819	24.001203
123.023751	5011.229322	24.006221
122.643759	5024.866511	24.011239
122.983963	5030.352161	24.016256
123.199117	5047.194453	24.021274
123.023919	5055.217445	24.026291
123.539070	5071.904280	24.031309
123.008190	5091.354351	24.036327
123.405801	5097.004963	24.041344
123.730398	5109.861968	24.046362
123.992127	5109.284888	24.051379
124.327669	5116.093107	24.056397
124.348386	5126.049684	24.061415
125.027317	5134.316661	24.066432
124.683795	5138.973901	24.071450
124.795459	5138.974814	24.076467
125.126807	5137.935402	24.081485
125.254357	5141.478100	24.086503
125.234683	5128.362147	24.091520
125.301463	5139.868740	24.096538
125.677978	5157.060506	24.101555
125.826700	5166.350625	24.106573
125.872911	5168.164091	24.111591
126.378937	5158.790339	24.116608
126.537138	5150.049312	24.121626
126.677598	5163.239570	24.126643
126.829880	5155.486222	24.131661
126.691795	5153.237644	24.136679
126.411955	5167.379321	24.141696
126.591033	5153.340662	24.146714
126.503048	5154.188023	24.151731
126.939998	5164.087662	24.156749
126.722262	5180.854368	24.161767
126.704627	5184.119856	24.166784
126.974624	5186.344815	24.171802
127.002823	5211.778808	24.176819
127.183356	5205.751638	24.181837
127.269475	5224.347886	24.186855
127.290574	5243.621894	24.191872
127.824910	5249.615360	24.196890
127.575637	5263.249269	24.201907
127.638410	5273.167885	24.206925
127.557091	5272.691974	24.211943
127.976296	5295.277761	24.216960
128.461214	5310.075171	24.221978
128.454656	5312.676585	24.226995
128.806093	5316.484722	24.232013
129.044790	5330.386915	24.237031
128.963682	5333.261307	24.242048
129.135567	5341.457435	24.247066
129.299435	5344.561457	24.252083
129.294583	5345.697878	24.257101
129.295351	5358.588121	24.262119
129.491873	5374.145522	24.267136
129.833708	5366.806859	24.272154
129.616865	5377.745466	24.277171
129.873457	5395.658958	24.282189
129.972781	5392.016252	24.287207
130.367684	5402.433673	24.292224
130.817897	5409.013997	24.297242
130.647475	5421.438430	24.302259
130.931938	5421.865959	24.307277
131.088541	5445.079667	24.312295
131.214308	5437.283705	24.317312
131.295716	5428.546156	24.322330
131.105656	5439.442188	24.327347
131.290296	5431.188815	24.332365
131.765906	5444.142417	24.337383
131.827625	5452.787562	24.342400
131.902411	5453.445033	24.347418
131.651310	5459.943598	24.352435
132.266346	5461.638699	24.357453
131.798121	5469.113010	24.362471
131.991580	5494.583156	24.367488
132.192309	5494.993416	24.372506
132.143599	5503.204422	24.377523
132.603135	5517.692015	24.382541
132.536769	5520.893177	24.387559
132.651337	5526.077270	24.392576
133.169459	5537.511942	24.397594
133.174812	5555.745115	24.402611
133.611470	5541.214679	24.407629
133.434287	5546.802932	24.412647
133.298448	5558.858725	24.417664
133.720588	5547.332211	24.422682
134.006236	5569.913688	24.427699
134.009182	5580.622003	24.432717
133.871486	5571.389413	24.437735
134.177141	5580.576673	24.442752
134.644337	5567.984308	24.447770
134.213349	5587.981544	24.452787
134.753447	5608.105395	24.457805
134.651002	5615.691011	24.462823
134.622116	5606.633751	24.467840
135.101251	5622.241172	24.472858
135.016756	5631.201554	24.477875
135.371878	5632.479722	24.482893
135.138585	5631.619807	24.487911
135.144281	5654.921366	24.492928
135.818732	5663.339385	24.497946
135.763597	5676.654531	24.502963
135.757616	5658.751424	24.507981
136.355501	5681.826420	24.512999
136.395544	5692.351495	24.518016
136.768009	5689.862162	24.523034
136.753906	5696.554765	24.528051
136.707475	5691.414229	24.533069
136.685806	5699.036545	24.538087
136.966345	5711.009876	24.543104
137.217637	5704.889711	24.548122
137.171707	5721.176975	24.553139
137.363748	5724.226412	24.558157
137.396160	5722.850481	24.563175
137.446294	5750.328046	24.568192
137.839392	5744.992412	24.573210
138.080944	5749.002695	24.578227
138.110506	5746.517249	24.583245
138.563854	5764.659711	24.588263
138.581109	5775.874522	24.593280
138.784852	5762.152940	24.598298
139.265446	5768.227151	24.603315
139.214885	5773.653599	24.608333
139.134288	5758.187431	24.613351
138.956669	5772.567125	24.618368
139.136376	5777.387344	24.623386
139.154518	5792.206032	24.628403
139.319922	5807.524486	24.633421
139.626598	5798.101000	24.638439
139.697641	5810.659488	24.643456
140.014818	5819.484703	24.648474
139.894343	5826.930861	24.653491
140.185638	5833.310428	24.658509
140.429800	5838.478725	24.663527
140.421156	5851.904465	24.668544
140.407222	5867.118733	24.673562
140.462443	5876.835409	24.678579
140.559590	5881.767740	24.683597
140.835904	5897.599525	24.688615
140.834378	5909.816886	24.693632
140.938332	5907.786903	24.698650
140.852538	5947.281846	24.703667
140.866209	5943.655920	24.708685
141.532005	5950.857639	24.713703
141.547815	5962.187405	24.718720
141.866780	5963.839739	24.723738
142.064350	5978.630531	24.728755
142.383798	5992.641641	24.733773
142.596798	5989.003246	24.738791
142.751174	5999.008776	24.743808
142.858481	5992.858345	24.748826
142.766260	6001.547735	24.753843
142.943165	6002.478950	24.758861
143.279968	6004.880812	24.763879
143.201551	6028.249587	24.768896
143.563957	6028.573298	24.773914
143.652546	6034.345008	24.778931
143.691530	6036.420832	24.783949
143.931891	6026.286408	24.788967
143.978395	6020.959123	24.793984
143.813474	6029.660540	24.799002
143.777496	6050.819260	24.804019
143.845639	6053.569108	24.809037
144.479282	6056.670466	24.814055
144.240767	6088.127211	24.819072
144.562361	6086.761350	24.824090
145.414585	6070.586725	24.829107
145.912161	6078.892442	24.834125
146.218038	6075.646222	24.839143
145.825696	6083.654034	24.844160
146.499357	6078.809807	24.849178
146.586898	6068.612010	24.854195
146.555020	6058.178008	24.859213
146.466160	6041.498966	24.864231
146.324421	6051.626303	24.869248
146.551522	6059.991664	24.874266
146.502736	6079.964175	24.879283
146.615934	6084.685619	24.884301
147.029952	6069.872567	24.889319
146.477077	6083.110039	24.894336
146.815181	6089.299273	24.899354
146.829957	6104.590536	24.904371
147.017516	6111.893006	24.909389
147.203440	6127.578912	24.914407
147.100130	6139.178920	24.919424
147.157913	6153.796094	24.924442
147.602864	6167.779144	24.929459
147.663364	6179.398579	24.934477
147.775079	6186.687627	24.939495
147.953221	6200.597449	24.944512
148.299917	6208.936829	24.949530
148.599963	6223.629806	24.954547
148.285116	6239.201683	24.959565
148.862840	6241.972895	24.964583
148.947922	6263.277279	24.969600
149.002331	6268.802321	24.974618
149.050161	6282.857389	24.979635
149.303767	6292.095015	24.984653
149.231480	6300.265050	24.989671
149.284723	6318.571131	24.994688
149.706558	6332.629025	24.999706
150.088688	6327.513155	25.004723
150.302614	6340.364259	25.009741
150.826883	6352.147392	25.014759
150.653368	6355.660964	25.019776
151.059446	6361.992644	25.024794
151.600938	6354.068080	25.029811
151.222502	6352.799749	25.034829
151.517989	6350.624659	25.039847
151.584280	6355.706749	25.044864
151.763941	6345.132862	25.049882
151.693635	6369.296606	25.054899
151.741567	6372.983864	25.059917
152.414895	6375.543209	25.064935
152.048498	6387.479832	25.069952
152.359704	6376.654229	25.074970
152.578338	6377.589204	25.079987
152.519768	6390.355430	25.085005
152.683995	6400.135536	25.090023
152.352115	6415.961626	25.095040
152.775581	6410.639653	25.100058
153.047129	6416.165095	25.105075
153.348870	6440.116268	25.110093
153.604260	6441.710643	25.115111
153.766788	6444.170114	25.120128
153.601972	6440.883461	25.125146
153.884462	6461.440413	25.130163
153.731114	6472.225957	25.135181
154.198161	6478.776784	25.140199
154.181466	6485.244522	25.145216
154.194750	6490.826051	25.150234
154.456304	6496.173615	25.155251
154.438556	6510.620892	25.160269
154.403442	6516.421488	25.165287
155.106204	6531.390006	25.170304
155.118551	6536.156602	25.175322
155.485917	6558.696863	25.180339
155.514606	6559.933361	25.185357
155.784547	6558.802021	25.190375
155.678548	6568.241771	25.195392
156.198000	6585.433938	25.200410
155.924959	6588.244978	25.205427
155.984950	6590.582806	25.210445
156.282465	6603.225792	25.215463
156.464720	6616.665139	25.220480
156.790349	6609.540822	25.225498
157.215789	6617.687850	25.230515
157.462211	6635.592235	25.235533
157.351749	6643.492326	25.240551
157.694885	6646.561477	25.245568
157.840193	6647.499133	25.250586
158.124168	6651.928703	25.255603
158.179141	6670.173479	25.260621
158.544439	6672.389996	25.265639
158.752388	6675.957167	25.270656
158.860422	6681.491608	25.275674
158.638288	6681.234625	25.280691
158.445209	6676.704326	25.285709
158.908089	6696.774216	25.290727
158.967082	6713.236940	25.295744
158.888958	6704.704996	25.300762
159.172224	6729.685842	25.305779
159.304531	6733.084388	25.310797
159.496331	6727.278440	25.315815
159.779257	6755.809665	25.320832
159.765183	6766.925222	25.325850
160.314854	6766.446209	25.330867
160.131032	6776.143871	25.335885
160.250052	6794.088389	25.340903
160.671563	6799.740400	25.345920
160.610935	6803.808759	25.350938
161.158269	6822.039302	25.355955
160.781554	6832.179187	25.360973
161.033992	6833.635481	25.365991
161.160420	6849.295710	25.371008
161.554374	6855.198801	25.376026
162.038625	6854.395095	25.381043
162.077516	6868.271812	25.386061
162.295128	6886.578961	25.391079
162.182397	6885.939258	25.396096
162.192833	6887.376475	25.401114
162.720564	6892.692796	25.406131
162.706406	6920.378738	25.411149
162.860862	6914.647410	25.416167
163.344328	6917.113783	25.421184
163.303527	6914.765788	25.426202
163.050976	6920.358316	25.431219
163.244230	6945.400055	25.436237
163.410434	6939.270633	25.441255
164.068958	6947.410824	25.446272
163.872093	6970.956901	25.451290
164.189839	6971.647144	25.456307
164.053108	6979.591122	25.461325
164.342885	6992.806684	25.466343
164.298342	7004.749661	25.471360
164.447820	7008.956622	25.476378
164.519349	7030.854959	25.481395
164.906018	7052.118457	25.486413
164.988788	7049.003411	25.491431
164.940149	7074.654734	25.496448
165.090572	7081.740910	25.501466
165.684211	7085.712266	25.506483
165.627656	7111.863488	25.511501
166.049748	7109.152307	25.516519
166.073748	7135.057137	25.521536
166.043842	7142.063663	25.526554
166.547376	7148.301591	25.531571
166.970491	7159.529482	25.536589
167.173933	7168.026143	25.541607
167.437944	7154.675759	25.546624
167.244712	7169.199100	25.551642
167.740563	7175.909278	25.556659
167.740624	7196.579225	25.561677
167.903721	7196.919358	25.566695
168.036567	7194.243352	25.571712
168.002026	7219.766569	25.576730
168.059444	7212.279909	25.581747
168.437494	7226.500205	25.586765
168.761071	7246.626105	25.591783
169.007665	7254.239897	25.596800
168.832261	7267.133248	25.601818
169.369754	7259.289229	25.606835
169.218907	7277.917612	25.611853
169.302034	7280.969993	25.616871
169.794378	7283.264054	25.621888
169.700287	7312.485494	25.626906
170.021064	7322.011122	25.631923
170.091491	7318.282961	25.636941
170.464745	7324.770885	25.641959
170.709342	7342.918164	25.646976
170.967410	7348.638335	25.651994
171.178021	7336.381121	25.657011
171.129044	7348.652724	25.662029
171.435823	7362.309196	25.667047
171.220605	7368.949499	25.672064
171.114148	7378.590643	25.677082
171.767602	7375.141816	25.682100
171.726353	7400.769608	25.687117
172.181447	7412.897332	25.692135
172.543446	7421.436453	25.697152
172.279101	7427.475306	25.702170
172.892704	7437.955219	25.707188
172.950884	7435.383657	25.712205
173.189217	7433.332853	25.717223
173.153205	7447.513864	25.722240
173.146933	7462.772119	25.727258
173.427225	7456.856773	25.732276
173.414385	7476.160391	25.737293
173.716789	7482.720730	25.742311
174.173084	7487.129942	25.747328
173.858303	7502.050140	25.752346
174.334110	7503.078947	25.757364
174.446328	7518.254671	25.762381
174.394688	7524.661663	25.767399
175.018469	7532.025823	25.772416
174.959310	7549.985676	25.777434
174.939776	7551.970557	25.782452
175.199061	7557.133775	25.787469
174.938194	7571.945106	25.792487
175.520532	7585.109677	25.797504
175.392535	7591.620673	25.802522
175.573649	7613.847467	25.807540
175.852965	7624.744245	25.812557
175.603617	7645.570189	25.817575
176.308624	7645.619958	25.822592
176.381620	7683.982899	25.827610
176.767671	7690.420816	25.832628
176.739373	7690.996572	25.837645
177.149176	7709.980975	25.842663
177.138621	7718.478637	25.847680
177.436031	7723.675778	25.852698
177.660333	7747.524383	25.857716
177.608820	7761.880722	25.862733
177.952237	7770.653871	25.867751
178.226175	7781.720980	25.872768
178.562945	7787.635447	25.877786
178.671068	7792.417314	25.882804
178.772730	7809.222253	25.887821
179.034453	7816.289583	25.892839
179.274827	7814.990557	25.897856
179.305078	7840.370966	25.902874
179.820446	7840.554459	25.907892
179.860617	7847.550507	25.912909
180.142128	7864.391948	25.917927
180.258393	7877.914160	25.922944
180.100617	7882.440696	25.927962
180.777955	7885.804573	25.932980
181.190134	7896.734719	25.937997
181.369233	7900.151779	25.943015
181.448593	7898.542252	25.948032
181.408750	7905.594077	25.953050
181.848900	7888.674453	25.958068
182.077888	7902.877459	25.963085
182.026484	7925.209268	25.968103
182.499909	7923.495249	25.973120
182.326708	7922.652839	25.978138
182.453608	7919.902871	25.983156
182.517855	7933.050158	25.988173
182.498674	7939.609477	25.993191
182.884806	7950.414797	25.998208
182.937657	7956.082458	26.003226
183.158892	7978.363783	26.008244
183.385339	7977.260010	26.013261
183.160597	7992.241402	26.018279
183.529681	8015.787676	26.023296
183.434115	8020.252778	26.028314
183.681338	8046.905111	26.033332
183.978974	8060.400663	26.038349
183.925487	8080.298508	26.043367
184.521486	8096.124191	26.048384
184.607202	8113.785080	26.053402
184.578325	8111.883093	26.058420
184.901361	8138.786121	26.063437
184.941855	8148.968178	26.068455
185.898685	8158.699546	26.073472
185.650195	8172.933640	26.078490
185.885828	8173.085384	26.083508
186.103502	8182.406459	26.088525
186.111524	8202.192691	26.093543
186.241967	8200.625889	26.098560
186.421007	8220.265744	26.103578
186.649820	8243.844985	26.108596
186.946679	8247.349781	26.113613
187.239985	8257.195566	26.118631
187.431817	8262.245715	26.123648
187.332962	8277.118362	26.128666
187.735656	8286.957119	26.133684
187.874805	8300.621623	26.138701
187.941545	8312.230572	26.143719
188.156340	8324.160838	26.148736
188.306208	8342.820339	26.153754
188.313459	8354.833752	26.158772
188.434183	8364.161500	26.163789
188.663854	8367.604962	26.168807
189.456980	8397.084296	26.173824
189.223854	8420.764540	26.178842
189.602994	8400.036783	26.183860
189.847875	8426.421560	26.188877
190.176669	8437.431233	26.193895
190.823897	8433.150682	26.198912
190.394716	8441.573760	26.203930
190.960834	8453.211361	26.208948
191.074604	8456.633823	26.213965
191.079206	8458.610103	26.218983
191.571199	8457.541976	26.224000
191.284533	8484.422668	26.229018
191.614719	8494.126246	26.234036
191.915313	8494.698887	26.239053
191.712866	8518.193838	26.244071
192.386665	8510.866221	26.249088
192.241011	8525.590880	26.254106
192.459152	8548.107447	26.259124
193.038941	8551.975927	26.264141
193.162113	8551.533471	26.269159
193.373261	8565.009087	26.274176
193.388872	8580.961868	26.279194
193.252043	8587.583426	26.284212
193.762141	8576.497410	26.289229
194.225362	8603.867194	26.294247
194.078752	8597.683272	26.299264
194.330005	8615.540274	26.304282
194.720442	8628.488531	26.309300
195.055259	8641.085246	26.314317
194.847928	8650.899783	26.319335
195.471987	8653.807921	26.324352
195.176963	8672.584637	26.329370
195.358455	8673.835437	26.334388
195.612279	8691.473133	26.339405
195.852008	8688.473610	26.344423
195.960219	8705.273693	26.349440
196.177063	8727.689910	26.354458
196.368019	8738.713116	26.359476
196.610914	8751.516505	26.364493
196.776696	8770.344801	26.369511
196.865126	8767.140266	26.374528
197.342501	8790.482341	26.379546
197.282199	8805.533423	26.384564
197.788430	8811.980301	26.389581
197.600496	8829.923498	26.394599
197.971319	8838.113000	26.399616
198.397628	8852.927773	26.404634
198.273205	8856.232931	26.409652
198.866072	8857.561495	26.414669
198.580434	8887.497235	26.419687
198.936774	8886.975287	26.424704
199.407908	8893.595769	26.429722
199.838948	8915.779160	26.434740
200.469185	8913.986359	26.439757
200.419020	8917.350151	26.444775
200.773511	8918.198249	26.449792
200.794602	8913.715411	26.454810
200.593584	8917.945348	26.459828
200.715386	8916.074293	26.464845
201.003577	8916.942009	26.469863
201.187928	8914.508470	26.474880
201.255581	8937.198534	26.479898
201.022857	8940.446776	26.484916
201.339307	8944.325781	26.489933
201.508127	8966.384009	26.494951
201.713493	8980.174424	26.499968
201.926234	8996.043854	26.504986
201.691642	9014.733797	26.510004
202.264239	9038.649678	26.515021
202.216985	9058.359467	26.520039
202.874099	9067.912500	26.525056
202.787888	9079.583514	26.530074
202.451034	9100.722773	26.535092
202.815403	9124.455003	26.540109
203.431540	9146.918479	26.545127
203.575598	9153.484411	26.550144
204.016816	9176.710152	26.555162
204.002878	9186.978273	26.560180
204.585593	9204.197508	26.565197
204.579427	9218.657946	26.570215
204.640780	9241.156504	26.575232
204.739159	9251.146176	26.580250
205.166485	9270.994429	26.585268
205.745773	9278.243100	26.590285
205.331289	9304.101044	26.595303
205.639354	9307.284429	26.600320
206.006441	9328.986665	26.605338
206.261331	9349.186455	26.610356
206.695440	9370.898943	26.615373
206.769375	9384.714575	26.620391
207.087317	9384.113888	26.625408
207.597355	9402.724580	26.630426
207.343560	9418.881825	26.635444
207.904485	9418.835693	26.640461
208.273061	9443.558613	26.645479
208.193408	9449.440109	26.650496
208.315889	9449.263193	26.655514
208.520179	9469.168236	26.660532
208.600092	9470.094815	26.665549
208.451484	9496.139935	26.670567
208.874380	9504.191998	26.675584
209.303263	9526.489240	26.680602
209.081773	9534.256301	26.685620
209.791154	9541.786073	26.690637
209.838991	9573.588395	26.695655
210.121078	9582.451455	26.700672
210.494661	9589.375856	26.705690
210.810555	9601.310860	26.710708
211.151118	9620.102621	26.715725
211.343599	9629.960405	26.720743
211.161847	9628.135481	26.725760
211.725668	9646.715519	26.730778
211.344894	9667.944705	26.735796
212.190094	9678.253943	26.740813
212.339165	9702.148639	26.745831
212.433578	9704.582068	26.750848
212.507055	9715.740366	26.755866
212.824785	9733.523839	26.760884
212.745051	9735.213310	26.765901
212.807024	9750.549136	26.770919
213.372765	9755.210303	26.775936
214.129209	9774.500680	26.780954
213.962093	9782.910308	26.785972
214.342943	9796.403832	26.790989
214.453576	9793.745241	26.796007
214.719737	9794.333863	26.801024
215.056690	9807.109962	26.806042
214.724779	9814.016324	26.811060
215.194504	9816.133333	26.816077
215.274448	9837.617461	26.821095
215.610572	9844.945954	26.826112
215.905547	9858.728629	26.831130
215.860641	9871.523758	26.836148
215.726635	9880.547105	26.841165
215.869252	9891.708282	26.846183
216.011330	9920.932523	26.851200
216.862182	9930.700624	26.856218
216.514783	9948.292535	26.861236
217.142753	9962.646514	26.866253
217.202014	9977.783715	26.871271
217.152874	9986.132997	26.876288
217.630427	10007.700540	26.881306
217.393914	10024.957554	26.886324
217.978861	10039.987481	26.891341
218.288825	10063.006190	26.896359
218.620623	10080.090596	26.901376
219.040748	10085.833038	26.906394
218.933022	10120.030031	26.911412
219.265905	10118.546180	26.916429
219.653340	10138.209116	26.921447
219.754943	10150.834534	26.926464
219.898075	10155.153665	26.931482
220.006431	10174.953343	26.936500
220.724275	10188.097703	26.941517
220.719461	10207.377316	26.946535
220.971022	10210.778967	26.951552
220.989519	10226.038146	26.956570
221.300985	10241.679822	26.961588
221.820734	10262.092234	26.966605
222.112568	10278.576119	26.971623
222.034200	10279.947180	26.976640
222.399590	10300.283527	26.981658
222.270176	10300.106471	26.986676
222.885875	10318.712597	26.991693
223.182008	10344.336656	26.996711
223.017158	10347.384123	27.001728
223.592570	10360.122844	27.006746
223.588359	10375.453662	27.011764
223.722222	10386.634750	27.016781
223.872476	10398.374004	27.021799
224.039679	10425.794259	27.026816
224.432830	10436.334652	27.031834
224.380392	10458.142401	27.036852
224.916911	10476.478208	27.041869
225.357760	10484.541984	27.046887
225.118982	10499.466604	27.051904
225.849929	10511.477087	27.056922
225.627640	10529.843794	27.061940
226.077728	10526.946243	27.066957
226.156525	10553.851175	27.071975
226.044892	10562.979918	27.076992
226.695748	10582.318657	27.082010
227.001192	10604.225813	27.087028
227.044326	10624.798573	27.092045
227.359647	10633.179356	27.097063
227.413446	10661.389953	27.102080
227.844157	10668.534622	27.107098
227.944753	10689.401253	27.112116
228.177396	10703.915747	27.117133
228.645675	10731.919347	27.122151
228.357001	10752.167394	27.127168
229.037315	10746.530570	27.132186
229.604544	10764.993189	27.137204
229.499087	10780.730272	27.142221
229.967311	10784.067891	27.147239
230.050318	10804.117528	27.152256
230.242350	10801.594208	27.157274
230.426359	10820.011495	27.162292
230.593185	10826.134002	27.167309
230.973025	10824.128714	27.172327
230.860115	10833.431128	27.177344
231.614479	10858.710106	27.182362
231.548524	10886.302015	27.187380
231.828458	10889.061828	27.192397
231.907805	10907.312172	27.197415
231.962933	10912.590571	27.202432
232.250912	10933.346210	27.207450
232.325700	10953.233537	27.212468
232.805983	10963.865445	27.217485
233.260791	10975.884878	27.222503
233.149411	11012.093172	27.227520
233.563628	11010.713181	27.232538
233.677666	11026.712016	27.237556
233.632463	11036.117587	27.242573
234.256486	11057.189692	27.247591
234.111913	11090.985207	27.252608
234.959765	11093.781997	27.257626
234.915545	11108.086576	27.262644
235.373145	11111.413416	27.267661
235.850369	11140.747583	27.272679
236.109286	11149.968267	27.277696
236.317903	11153.469385	27.282714
236.208828	11169.413054	27.287732
236.497433	11190.350111	27.292749
236.925345	11189.156121	27.297767
237.097016	11204.238886	27.302784
237.573332	11215.471112	27.307802
237.801193	11227.510899	27.312820
237.834429	11230.984290	27.317837
237.815845	11257.711912	27.322855
238.334788	11267.927205	27.327872
238.434853	11281.943407	27.332890
238.368490	11296.255750	27.337908
238.637102	11314.431173	27.342925
238.854909	11331.962729	27.347943
238.703781	11353.006523	27.352960
239.612459	11366.214077	27.357978
239.662834	11396.425922	27.362996
240.307729	11392.617657	27.368013
240.710773	11406.435809	27.373031
240.698912	11418.985652	27.378048
241.205532	11428.239624	27.383066
241.217825	11451.467858	27.388084
241.617415	11459.982470	27.393101
241.828422	11471.213018	27.398119
241.690690	11490.004073	27.403136
241.679589	11490.221831	27.408154
242.038897	11511.536006	27.413172
242.498489	11529.763626	27.418189
243.048775	11542.663429	27.423207
243.030425	11558.974574	27.428224
243.326798	11580.299238	27.433242
243.486751	11589.349031	27.438260
243.196844	11594.178896	27.443277
243.837788	11613.786011	27.448295
243.901547	11638.735218	27.453312
244.364712	11656.666970	27.458330
244.633866	11678.189271	27.463348
244.701244	11675.932990	27.468365
244.814560	11696.711386	27.473383
245.169267	11724.210025	27.478400
245.277361	11727.824777	27.483418
245.631829	11745.304270	27.488436
245.878041	11762.299051	27.493453
246.314199	11773.883362	27.498471
246.421933	11791.620315	27.503488
246.896928	11802.020467	27.508506
247.120692	11811.983148	27.513524
247.227087	11835.422488	27.518541
247.659774	11837.896469	27.523559
247.707259	11860.512082	27.528576
248.076370	11875.938642	27.533594
248.044422	11889.214588	27.538612
248.341825	11909.631179	27.543629
248.742292	11926.586468	27.548647
248.671085	11952.866223	27.553664
249.112855	11958.513596	27.558682
249.287475	11984.161143	27.563700
249.330034	12016.318186	27.568717
249.801733	12023.739519	27.573735
250.074405	12054.639874	27.578752
250.312830	12062.838735	27.583770
250.602807	12072.472361	27.588788
250.881716	12091.209464	27.593805
250.882616	12103.590715	27.598823
251.155329	12140.021705	27.603840
251.504231	12151.899594	27.608858
251.870221	12174.305463	27.613876
252.294678	12187.987611	27.618893
252.841680	12196.650007	27.623911
252.788157	12214.500728	27.628928
253.317246	12243.757440	27.633946
253.221322	12243.753663	27.638964
253.270570	12272.645371	27.643981
253.856440	12279.123841	27.648999
254.133351	12307.285499	27.654016
254.180956	12312.793284	27.659034
254.634073	12341.042488	27.664052
254.787399	12352.644009	27.669069
255.543071	12359.017251	27.674087
255.796483	12367.042832	27.679104
255.886587	12384.988188	27.684122
256.207482	12408.808112	27.689140
256.307502	12411.089765	27.694157
257.169054	12417.899330	27.699175
256.977236	12440.831823	27.704192
257.438605	12446.847201	27.709210
257.550861	12459.342684	27.714228
257.344849	12463.688609	27.719245
257.939926	12486.428136	27.724263
257.914328	12505.413776	27.729280
258.125425	12512.547499	27.734298
258.611250	12534.065088	27.739316
258.627827	12549.208616	27.744333
259.105041	12569.558521	27.749351
259.046795	12586.417756	27.754368
259.374672	12594.557203	27.759386
259.685560	12610.068145	27.764404
259.790316	12628.978821	27.769421
260.353568	12650.274207	27.774439
260.728542	12661.335111	27.779456
260.883898	12678.813852	27.784474
261.353926	12691.212591	27.789492
261.353789	12711.075866	27.794509
261.474444	12731.295800	27.799527
261.824039	12745.351625	27.804544
261.791008	12753.235640	27.809562
262.098589	12765.938597	27.814580
262.569345	12798.485774	27.819597
262.734640	12788.767971	27.824615
263.119587	12820.506853	27.829632
263.322646	12836.315515	27.834650
263.692430	12842.470654	27.839668
263.936855	12870.043047	27.844685
263.892427	12876.665286	27.849703
263.777595	12899.390321	27.854720
264.273012	12928.125190	27.859738
264.704919	12942.548912	27.864756
264.454469	12971.243208	27.869773
264.859994	12994.651360	27.874791
264.891525	13025.316089	27.879808
265.575994	13045.878170	27.884826
265.707393	13066.917703	27.889844
266.285172	13097.063724	27.894861
266.673671	13114.488661	27.899879
266.613308	13135.988564	27.904896
266.899872	13157.706934	27.909914
267.582896	13178.872931	27.914932
267.327796	13190.644953	27.919949
267.815875	13217.734902	27.924967
268.149714	13248.496653	27.929984
268.425270	13264.851572	27.935002
268.280633	13282.572768	27.940020
268.777325	13323.773888	27.945037
269.561039	13328.332349	27.950055
269.665543	13354.983232	27.955072
269.786254	13379.600329	27.960090
270.502102	13385.876565	27.965108
270.214566	13418.671603	27.970125
270.541420	13437.021015	27.975143
271.263944	13457.788487	27.980160
271.246189	13481.821945	27.985178
271.780630	13485.808659	27.990196
272.009713	13511.405514	27.995213
272.520487	13539.754447	28.000231
272.560974	13553.498041	28.005248
272.933421	13568.111785	28.010266
273.183454	13593.918039	28.015284
272.865808	13610.665981	28.020301
273.507178	13623.097011	28.025319
273.775278	13641.977947	28.030336
274.175568	13664.888412	28.035354
274.378930	13675.308656	28.040372
274.795965	13698.249493	28.045389
275.325652	13703.546529	28.050407
275.737524	13720.096847	28.055424
275.704282	13735.965914	28.060442
275.692439	13746.568306	28.065460
275.853092	13777.610227	28.070477
276.503798	13802.751817	28.075495
276.741737	13814.461746	28.080512
276.829308	13827.638384	28.085530
277.007297	13845.993945	28.090548
277.236527	13882.402957	28.095565
277.521439	13894.670899	28.100583
277.678787	13923.376720	28.105600
277.622685	13947.841097	28.110618
278.593219	13968.936995	28.115636
278.668373	13993.579885	28.120653
278.822563	14007.421689	28.125671
279.201893	14031.915108	28.130688
279.165664	14062.853005	28.135706
279.521520	14065.403852	28.140724
279.543996	14101.009172	28.145741
279.942795	14127.158866	28.150759
280.284928	14153.380998	28.155776
280.382010	14180.586006	28.160794
281.074065	14195.984285	28.165812
281.272826	14224.890233	28.170829
281.884541	14236.453621	28.175847
282.024404	14259.546627	28.180864
282.068786	14280.652538	28.185882
282.295469	14291.857249	28.190900
282.615127	14313.959362	28.195917
283.036268	14326.398954	28.200935
283.337944	14346.832104	28.205952
283.483633	14384.582912	28.210970
284.095755	14391.068936	28.215988
284.484468	14430.762130	28.221005
284.620400	14438.407883	28.226023
284.575390	14466.352285	28.231040
284.666527	14479.724271	28.236058
285.252965	14492.700843	28.241076
285.497754	14542.618675	28.246093
285.799236	14557.602760	28.251111
286.263708	14578.370182	28.256128
286.316690	14602.423552	28.261146
286.821892	14621.072624	28.266164
287.263974	14646.372910	28.271181
287.245452	14670.769129	28.276199
288.101449	14687.839597	28.281216
287.949447	14716.216561	28.286234
288.357797	14715.465234	28.291252
288.944473	14743.598868	28.296269
288.951410	14783.420606	28.301287
289.515300	14776.106770	28.306304
289.480304	14806.292599	28.311322
289.616804	14830.338812	28.316340
289.579050	14854.957534	28.321357
289.844046	14879.222128	28.326375
290.534985	14906.916478	28.331392
290.638591	14930.158256	28.336410
290.868067	14956.319924	28.341428
291.031100	14994.965975	28.346445
291.519984	15012.957885	28.351463
292.461616	15027.805129	28.356480
292.838286	15061.650467	28.361498
293.574512	15062.925176	28.366516
293.605059	15073.207821	28.371533
293.714079	15084.095271	28.376551
294.174693	15103.234496	28.381568
294.273773	15111.288516	28.386586
294.700922	15136.079854	28.391604
295.011105	15147.971075	28.396621
294.881830	15158.998801	28.401639
295.309874	15178.283754	28.406656
295.477050	15206.663998	28.411674
296.138366	15220.482942	28.416692
296.308635	15244.658142	28.421709
296.028467	15276.451827	28.426727
296.529966	15291.650969	28.431744
297.099418	15307.741915	28.436762
297.591469	15317.767238	28.441780
297.497829	15342.542491	28.446797
297.743713	15364.150763	28.451815
297.814550	15379.692198	28.456832
298.049981	15410.428602	28.461850
298.297074	15432.763281	28.466868
298.633640	15456.455870	28.471885
298.891647	15490.216113	28.476903
299.157105	15513.964660	28.481920
299.397513	15540.358702	28.486938
299.699856	15571.971625	28.491956
299.956844	15593.056720	28.496973
299.887534	15621.708422	28.501991
300.855691	15641.654859	28.507008
300.692620	15679.757533	28.512026
301.311408	15692.696628	28.517044
301.412970	15726.877201	28.522061
301.663450	15744.406566	28.527079
302.346872	15772.702508	28.532096
302.395418	15798.055414	28.537114
303.043023	15814.157590	28.542132
303.574288	15843.566228	28.547149
304.166320	15859.674479	28.552167
304.188944	15873.336302	28.557184
303.920276	15902.385485	28.562202
304.832872	15922.828432	28.567220
305.033330	15926.363462	28.572237
305.332541	15959.862555	28.577255
305.396698	15972.748507	28.582272
305.371245	16005.089377	28.587290
305.586940	16039.064202	28.592308
306.032667	16061.797178	28.597325
306.227111	16095.376897	28.602343
306.674772	16119.337355	28.607360
306.921829	16146.539777	28.612378
307.311959	16174.424669	28.617396
307.671623	16206.610905	28.622413
307.839916	16227.249693	28.627431
308.537567	16266.940447	28.632448
308.862858	16287.937929	28.637466
309.159102	16314.439047	28.642484
309.708476	16339.766789	28.647501
310.092942	16354.515020	28.652519
310.417625	16387.943012	28.657536
310.702876	16404.899964	28.662554
310.991666	16422.407967	28.667572
311.274604	16450.861081	28.672589
311.502899	16468.632873	28.677607
311.984705	16475.073498	28.682624
312.272642	16501.867862	28.687642
312.482830	16514.481098	28.692660
312.968791	16542.273559	28.697677
313.128528	16575.724454	28.702695
313.583478	16590.905706	28.707712
313.705968	16615.599895	28.712730
313.522238	16633.056948	28.717748
314.315645	16656.329069	28.722765
314.770001	16688.714955	28.727783
315.259001	16698.331854	28.732800
315.236019	16724.690938	28.737818
315.480369	16748.985361	28.742836
315.697534	16765.895620	28.747853
316.130547	16787.002033	28.752871
316.665181	16795.232374	28.757888
316.959162	16853.308548	28.762906
317.019657	16860.246049	28.767924
317.427005	16885.571306	28.772941
317.776429	16916.368934	28.777959
318.094979	16935.303668	28.782976
318.134204	16972.074061	28.787994
318.391791	17003.003654	28.793012
318.708235	17026.730212	28.798029
318.791902	17042.822743	28.803047
319.434973	17082.671070	28.808064
319.364901	17109.432579	28.813082
319.617719	17140.560233	28.818100
320.017018	17168.982760	28.823117
320.386519	17209.637857	28.828135
320.529709	17237.971994	28.833152
320.989042	17266.679509	28.838170
321.477142	17287.755400	28.843188
322.167883	17324.105297	28.848205
322.074871	17331.771314	28.853223
322.963796	17356.754526	28.858240
323.140086	17385.915653	28.863258
323.509624	17408.469220	28.868276
323.995581	17426.412263	28.873293
324.097840	17451.410518	28.878311
324.466805	17467.325513	28.883328
324.464724	17498.770205	28.888346
324.484801	17517.575237	28.893364
325.263255	17543.610943	28.898381
325.487458	17581.037767	28.903399
325.800862	17606.195243	28.908416
326.160616	17627.921664	28.913434
326.370711	17652.210471	28.918452
327.076365	17678.780131	28.923469
327.023736	17697.966204	28.928487
327.863004	17725.199502	28.933504
328.101030	17742.327985	28.938522
328.533384	17771.036109	28.943540
329.010995	17791.578477	28.948557
328.992835	17800.085062	28.953575
329.687390	17827.829478	28.958592
329.896578	17855.256924	28.963610
329.866555	17873.268357	28.968628
330.237692	17900.134794	28.973645
330.477381	17941.114195	28.978663
331.114024	17964.248573	28.983680
331.024155	17996.709603	28.988698
331.285747	18020.006894	28.993716
331.923875	18040.734268	28.998733
332.327246	18075.818744	29.003751
332.670964	18093.420332	29.008768
332.823375	18127.777185	29.013786
332.832980	18154.779420	29.018804
333.188076	18195.893281	29.023821
333.781811	18217.897072	29.028839
334.017080	18250.401037	29.033856
334.507156	18284.204345	29.038874
334.928176	18314.291337	29.043892
335.347209	18345.154221	29.048909
335.381501	18376.302971	29.053927
335.434050	18402.322824	29.058944
335.806328	18429.717976	29.063962
335.966234	18465.827076	29.068980
336.436093	18505.021793	29.073997
337.165433	18537.001775	29.079015
337.433570	18556.310817	29.084032
337.893397	18596.809397	29.089050
338.177237	18632.918879	29.094068
338.410758	18648.745476	29.099085
338.743057	18690.860534	29.104103
339.259575	18727.771937	29.109120
340.019862	18753.793646	29.114138
339.837053	18777.163842	29.119156
340.285200	18807.882492	29.124173
340.308580	18835.430530	29.129191
341.028214	18867.281925	29.134208
341.123778	18909.476053	29.139226
341.412940	18928.901855	29.144244
341.882757	18965.468414	29.149261
342.191113	19004.557009	29.154279
342.550913	19016.042460	29.159296
343.025286	19045.871338	29.164314
342.822189	19079.521235	29.169332
343.496814	19111.823478	29.174349
343.719445	19136.649917	29.179367
344.209742	19158.977855	29.184384
344.786515	19188.044476	29.189402
344.995137	19217.320140	29.194420
345.562286	19258.095803	29.199437
345.695809	19267.552250	29.204455
346.330349	19276.703675	29.209472
346.481440	19309.406479	29.214490
346.791611	19352.791089	29.219508
347.116178	19359.662371	29.224525
347.774015	19394.094411	29.229543
348.094260	19424.617800	29.234560
348.448250	19446.524115	29.239578
348.621201	19464.648770	29.244596
348.695653	19494.568166	29.249613
349.066092	19528.953383	29.254631
349.437959	19541.197007	29.259648
349.757359	19579.079223	29.264666
349.751755	19608.993134	29.269684
350.497146	19638.961166	29.274701
350.989809	19667.323703	29.279719
351.172981	19700.811735	29.284736
351.693197	19733.779127	29.289754
352.059246	19770.191202	29.294772
352.466943	19794.165186	29.299789
352.839602	19812.254076	29.304807
353.294504	19840.463933	29.309824
353.889274	19865.327722	29.314842
354.197245	19884.738926	29.319860
354.866822	19918.687743	29.324877
354.922063	19935.208679	29.329895
355.316803	19947.499269	29.334912
355.553534	19984.232690	29.339930
355.794497	20008.641237	29.344948
356.064729	20026.422544	29.349965
356.115883	20065.597110	29.354983
356.272815	20101.771739	29.360000
356.789913	20128.141607	29.365018
356.894906	20167.893942	29.370036
357.516189	20194.640806	29.375053
357.608032	20240.573447	29.380071
358.036602	20278.174382	29.385088
358.491181	20318.564528	29.390106
358.671910	20357.846065	29.395124
359.729212	20383.266369	29.400141
360.064049	20418.729702	29.405159
360.273197	20442.445781	29.410176
361.050029	20464.806964	29.415194
361.337886	20509.601306	29.420212
361.624993	20522.127652	29.425229
362.178369	20541.347744	29.430247
362.454583	20567.023476	29.435264
363.159446	20581.287464	29.440282
362.977118	20620.196071	29.445300
363.341636	20646.021289	29.450317
363.400370	20670.360015	29.455335
363.666548	20705.491633	29.460352
364.149426	20735.796656	29.465370
364.487994	20771.695227	29.470388
365.033789	20802.734070	29.475405
365.338040	20837.725677	29.480423
365.737641	20866.186032	29.485440
366.248072	20899.986577	29.490458
366.379440	20930.476138	29.495476
366.686140	20955.527875	29.500493
367.401358	20992.331086	29.505511
367.607564	21015.884510	29.510528
367.799806	21039.656254	29.515546
368.120898	21080.147543	29.520564
368.916634	21096.941426	29.525581
369.137187	21123.054440	29.530599
369.285381	21156.507030	29.535616
369.643729	21183.710385	29.540634
369.755109	21220.035270	29.545652
370.276596	21233.587576	29.550669
370.747574	21264.849313	29.555687
370.264573	21301.849567	29.560704
371.244787	21338.210905	29.565722
371.571535	21371.101564	29.570740
371.799119	21403.192028	29.575757
372.553414	21447.158250	29.580775
372.453385	21483.956906	29.585792
373.104046	21510.079875	29.590810
372.970867	21557.784340	29.595828
373.324104	21587.470671	29.600845
374.473929	21627.900482	29.605863
374.744119	21673.287334	29.610880
375.576155	21696.511310	29.615898
375.634365	21737.476437	29.620916
376.104490	21768.297819	29.625933
376.209651	21789.915666	29.630951
376.997443	21821.684212	29.635968
377.620677	21845.113157	29.640986
377.444711	21879.636047	29.646004
377.841727	21902.788704	29.651021
378.182890	21940.556016	29.656039
378.585636	21978.527655	29.661056
378.957608	22016.132389	29.666074
379.189247	22048.489861	29.671092
379.529573	22086.888274	29.676109
379.766698	22121.326079	29.681127
380.414852	22161.043871	29.686144
380.807921	22201.696251	29.691162
381.541690	22231.429648	29.696180
382.423269	22255.571684	29.701197
382.556327	22286.561639	29.706215
382.627680	22311.455628	29.711232
383.150753	22343.768679	29.716250
383.381604	22386.121090	29.721268
383.467909	22403.867515	29.726285
384.158133	22447.643562	29.731303
384.035589	22484.498577	29.736320
384.798348	22514.129935	29.741338
384.812653	22558.164552	29.746356
385.466521	22590.853784	29.751373
385.608952	22632.264401	29.756391
385.616529	22679.776940	29.761408
386.166122	22718.761849	29.766426
386.485470	22770.106428	29.771444
386.844341	22802.333966	29.776461
387.644835	22840.033728	29.781479
388.076916	22892.742789	29.786496
389.000448	22911.562326	29.791514
389.088952	22953.797778	29.796532
389.682845	22993.138639	29.801549
389.978486	23020.148786	29.806567
390.194130	23053.106815	29.811584
390.743245	23080.530848	29.816602
390.807086	23121.608778	29.821620
391.213870	23163.423233	29.826637
391.683235	23195.625387	29.831655
391.559737	23238.076313	29.836672
392.342019	23268.877263	29.841690
392.608815	23316.258901	29.846708
392.952455	23364.868847	29.851725
393.589332	23395.537954	29.856743
393.948564	23436.354998	29.861760
393.981150	23462.444356	29.866778
394.650016	23500.444842	29.871796
394.732265	23544.169651	29.876813
395.573015	23572.411932	29.881831
395.253072	23608.121035	29.886848
395.657067	23650.980953	29.891866
396.388083	23696.180452	29.896884
396.945104	23744.429857	29.901901
397.444148	23767.661254	29.906919
397.846357	23805.883072	29.911936
398.298103	23849.464065	29.916954
398.461360	23889.236074	29.921972
398.985961	23922.830651	29.926989
399.848343	23958.299458	29.932007
400.178726	23998.723703	29.937024
400.282675	24030.199426	29.942042
400.709611	24058.944491	29.947060
401.317393	24101.609481	29.952077
402.083390	24137.491934	29.957095
402.142622	24157.266106	29.962112
402.729029	24200.031058	29.967130
402.740685	24230.499064	29.972148
403.370250	24261.595108	29.977165
404.123967	24287.320635	29.982183
404.418708	24330.283891	29.987200
405.134234	24341.938153	29.992218
405.337377	24376.764602	29.997236
405.432539	24430.032380	30.002253
405.956744	24453.071347	30.007271
406.228853	24488.443247	30.012288
406.693370	24516.068074	30.017306
406.959144	24563.600013	30.022324
407.276707	24604.926608	30.027341
407.820143	24630.012511	30.032359
407.724251	24680.983661	30.037376
408.154975	24722.246120	30.042394
408.732554	24752.202140	30.047412
408.803937	24814.962890	30.052429
409.156352	24838.024450	30.057447
409.489976	24883.002621	30.062464
410.508351	24930.977356	30.067482
410.650375	24977.679393	30.072500
411.250927	25016.489304	30.077517
412.117918	25049.870294	30.082535
412.512196	25095.690516	30.087552
412.982109	25128.757228	30.092570
413.776277	25157.534953	30.097588
414.122487	25182.181189	30.102605
415.018055	25207.941451	30.107623
415.142000	25239.193769	30.112640
415.930748	25261.169892	30.117658
416.177964	25274.969455	30.122676
416.005628	25303.777776	30.127693
416.301329	25329.014440	30.132711
416.889091	25369.967114	30.137728
417.106490	25408.478526	30.142746
417.752045	25437.017931	30.147764
417.863343	25466.971813	30.152781
418.073163	25512.013096	30.157799
418.278373	25553.486707	30.162816
418.720721	25594.610594	30.167834
419.134027	25644.882361	30.172852
419.326556	25688.944546	30.177869
420.136681	25724.130796	30.182887
420.190739	25769.023447	30.187904
420.592868	25819.128843	30.192922
420.785753	25861.535630	30.197940
421.167345	25904.545282	30.202957
421.352386	25936.454255	30.207975
421.808824	25999.892192	30.212992
422.099052	26043.349371	30.218010
422.884728	26080.905832	30.223028
423.186721	26129.246712	30.228045
423.768693	26170.697432	30.233063
423.806450	26227.500100	30.238080
424.067822	26268.795855	30.243098
424.903015	26307.931077	30.248116
424.975486	26377.694459	30.253133
425.783558	26427.069091	30.258151
426.208350	26474.037599	30.263168
426.464354	26512.761170	30.268186
426.879815	26569.234490	30.273204
427.727453	26608.563894	30.278221
428.456021	26645.705238	30.283239
429.133428	26685.536042	30.288256
429.523186	26723.559878	30.293274
429.751872	26773.621021	30.298292
430.243578	26817.081577	30.303309
430.388828	26854.609902	30.308327
431.128911	26903.104539	30.313344
431.943466	26946.701338	30.318362
432.041415	26986.824113	30.323380
432.643380	27014.502829	30.328397
433.374043	27058.258859	30.333415
433.719942	27090.156026	30.338432
434.213381	27118.855843	30.343450
434.735314	27155.395296	30.348468
434.941050	27194.989785	30.353485
435.341018	27223.802996	30.358503
435.710340	27265.950707	30.363520
436.323109	27311.020053	30.368538
436.635260	27350.247211	30.373556
436.763633	27386.653453	30.378573
437.373633	27422.011886	30.383591
437.684968	27471.433730	30.388608
438.076300	27519.738537	30.393626
438.297479	27555.931093	30.398644
438.541881	27608.266244	30.403661
438.791268	27664.082980	30.408679
439.490658	27708.091860	30.413696
440.113846	27765.540997	30.418714
440.853977	27806.837070	30.423732
441.083661	27862.610390	30.428749
441.317553	27889.140085	30.433767
441.567838	27943.124955	30.438784
442.192907	27983.825377	30.443802
443.038237	28019.417434	30.448820
443.128247	28075.419542	30.453837
444.005033	28114.533094	30.458855
444.881930	28154.283885	30.463872
444.978549	28202.513115	30.468890
445.635190	28243.051220	30.473908
445.986443	28286.548153	30.478925
446.139081	28325.542071	30.483943
446.453194	28375.738859	30.488960
446.863476	28416.475783	30.493978
447.575954	28462.137307	30.498996
447.700691	28508.545836	30.504013
448.591181	28524.214817	30.509031
449.042722	28578.086415	30.514048
449.429462	28614.203373	30.519066
450.226610	28652.334516	30.524084
450.685508	28697.464450	30.529101
450.981968	28716.373513	30.534119
451.481401	28763.739706	30.539136
451.920609	28800.170137	30.544154
451.846264	28831.581612	30.549172
452.433750	28872.514304	30.554189
452.537424	28910.703785	30.559207
452.692668	28947.837555	30.564224
453.175065	28998.156612	30.569242
453.894824	29044.023512	30.574260
453.959005	29096.474955	30.579277
454.614469	29131.337288	30.584295
455.028631	29192.295626	30.589312
455.259889	29243.798805	30.594330
455.476853	29296.490594	30.599348
456.098072	29349.825535	30.604365
456.952883	29394.194739	30.609383
457.369285	29460.245058	30.614400
457.518807	29508.775175	30.619418
458.124139	29552.129219	30.624436
458.441799	29604.347898	30.629453
459.588759	29650.205775	30.634471
460.301892	29682.968210	30.639488
460.881170	29733.188224	30.644506
461.959868	29771.347883	30.649524
462.246895	29796.584651	30.654541
462.656923	29833.611984	30.659559
462.982705	29871.460894	30.664576
463.579756	29901.003127	30.669594
464.389396	29922.393447	30.674612
464.259818	29970.472524	30.679629
464.713451	30012.609851	30.684647
465.023470	30056.275769	30.689664
465.581514	30097.752508	30.694682
465.953360	30130.748823	30.699700
465.955910	30187.986741	30.704717
466.428927	30231.468441	30.709735
466.680336	30281.576998	30.714752
466.915895	30338.108127	30.719770
468.081638	30380.068780	30.724788
468.262037	30426.457465	30.729805
468.620979	30472.138516	30.734823
469.463919	30528.197679	30.739840
469.848205	30580.266318	30.744858
470.447725	30620.343055	30.749876
470.597650	30673.882941	30.754893
471.462299	30728.894939	30.759911
471.547820	30769.820374	30.764928
472.041743	30822.117698	30.769946
472.871160	30875.662693	30.774964
473.186548	30920.976692	30.779981
473.925256	30965.943264	30.784999
474.447581	31012.485244	30.790016
474.522320	31049.277145	30.795034
474.967478	31102.700173	30.800052
475.330065	31155.679549	30.805069
476.085053	31211.821689	30.810087
476.024287	31254.315145	30.815104
476.062153	31317.387428	30.820122
477.153067	31380.219746	30.825140
477.250988	31436.111480	30.830157
478.104478	31494.651753	30.835175
478.490698	31556.938574	30.840192
479.013181	31597.986219	30.845210
479.786226	31653.028878	30.850228
480.046656	31701.499447	30.855245
480.984367	31738.020899	30.860263
481.625372	31785.684271	30.865280
481.985840	31841.578100	30.870298
482.742396	31880.518084	30.875316
483.319410	31916.541057	30.880333
483.366850	31952.635801	30.885351
483.679721	32003.556280	30.890368
483.601320	32047.174592	30.895386
484.086717	32084.298364	30.900404
484.390370	32146.947969	30.905421
484.765980	32203.263221	30.910439
485.472685	32247.216140	30.915456
485.599706	32313.091569	30.920474
486.440497	32381.824576	30.925492
486.826151	32430.446846	30.930509
486.848463	32497.737960	30.935527
487.901161	32552.844523	30.940544
487.957777	32626.866598	30.945562
488.429399	32677.043438	30.950580
488.928873	32751.724876	30.955597
489.321530	32807.181048	30.960615
490.407537	32869.110831	30.965632
490.707689	32923.648723	30.970650
491.658764	32970.090372	30.975668
492.156223	33039.043568	30.980685
492.711675	33084.594845	30.985703
492.989701	33142.112414	30.990720
493.399340	33209.285471	30.995738
493.997905	33252.066091	31.000756
494.621080	33318.828823	31.005773
494.906620	33379.362327	31.010791
495.574413	33433.235262	31.015808
495.481302	33504.414463	31.020826
496.413573	33565.633754	31.025844
497.035048	33622.670195	31.030861
497.191956	33668.714771	31.035879
498.168981	33724.367589	31.040896
498.491133	33778.869779	31.045914
499.325529	33843.801076	31.050932
499.928811	33907.303552	31.055949
500.257035	33961.249960	31.060967
501.048638	34011.049584	31.065984
501.572040	34072.896664	31.071002
502.318399	34114.793546	31.076020
502.825095	34166.764235	31.081037
502.904854	34234.689855	31.086055
503.406715	34269.035603	31.091072
503.638470	34317.985095	31.096090
504.202330	34383.174467	31.101108
504.491086	34448.624088	31.106125
504.924134	34510.932535	31.111143
505.645216	34567.475938	31.116160
505.869240	34635.663253	31.121178
506.424612	34685.251353	31.126196
507.390026	34737.466649	31.131213
507.976135	34795.361531	31.136231
508.572856	34843.422294	31.141248
509.240711	34909.767113	31.146266
509.664512	34945.793177	31.151284
510.338744	34992.724486	31.156301
510.937072	35052.281152	31.161319
511.634458	35105.734597	31.166336
511.993038	35154.999934	31.171354
512.408283	35201.441281	31.176372
512.777151	35250.481137	31.181389
513.145050	35306.428867	31.186407
513.859435	35362.938040	31.191424
513.776277	35416.950502	31.196442
514.313029	35473.514610	31.201460
515.057913	35532.455420	31.206477
515.448051	35593.913259	31.211495
516.328827	35630.307019	31.216512
516.618285	35688.490476	31.221530
517.181207	35732.134993	31.226548
517.952146	35783.296778	31.231565
518.527026	35843.229174	31.236583
518.861039	35880.307022	31.241600
519.033024	35924.344771	31.246618
519.439897	35992.298796	31.251636
519.833931	36035.391299	31.256653
520.176843	36097.868501	31.261671
520.765029	36161.810695	31.266688
521.338130	36225.733520	31.271706
521.277437	36273.862542	31.276724
522.366037	36336.037533	31.281741
522.575836	36404.861952	31.286759
523.017965	36465.651485	31.291776
523.479430	36543.381540	31.296794
524.422006	36611.000122	31.301812
524.811540	36664.610067	31.306829
524.922581	36740.682086	31.311847
525.941789	36793.639299	31.316864
526.583844	36867.992577	31.321882
526.933117	36925.176074	31.326900
527.706139	36990.214186	31.331917
528.409289	37053.607229	31.336935
529.242881	37117.281919	31.341952
529.574931	37184.410192	31.346970
529.754837	37243.345807	31.351988
530.478939	37297.568283	31.357005
530.573416	37380.503596	31.362023
531.062019	37431.713568	31.367040
531.656345	37503.855562	31.372058
532.108793	37573.370251	31.377076
532.813023	37638.519906	31.382093
533.147240	37705.097462	31.387111
534.022027	37783.354784	31.392128
534.556435	37852.219494	31.397146
535.097429	37910.788360	31.402164
535.867672	37982.180480	31.407181
535.850086	38055.072739	31.412199
536.694428	38119.481407	31.417216
537.353977	38186.439388	31.422234
538.055474	38254.324895	31.427252
538.678455	38315.734652	31.432269
539.190596	38381.401603	31.437287
540.155293	38438.529285	31.442304
540.861917	38503.785822	31.447322
541.360788	38538.847238	31.452340
542.250755	38600.734633	31.457357
542.917832	38654.241535	31.462375
543.417362	38692.954836	31.467392
543.562218	38765.980937	31.472410
543.950230	38810.772802	31.477428
544.294215	38862.749270	31.482445
544.635278	38931.956181	31.487463
545.282894	38993.682950	31.492480
545.628872	39058.006837	31.497498
546.020488	39127.108299	31.502516
546.649447	39185.430045	31.507533
546.973577	39254.697796	31.512551
547.550726	39336.801692	31.517568
548.137487	39396.822859	31.522586
548.349962	39469.335612	31.527604
549.461496	39538.812121	31.532621
549.785226	39611.897299	31.537639
550.454552	39664.286310	31.542656
551.241511	39731.109015	31.547674
551.954495	39797.208748	31.552692
552.504313	39855.624627	31.557709
552.925847	39917.028890	31.562727
553.476520	39973.513293	31.567744
553.976389	40032.727091	31.572762
554.512648	40094.255042	31.577780
555.232455	40133.556849	31.582797
555.499943	40206.584262	31.587815
556.253081	40253.800343	31.592832
556.480283	40315.380085	31.597850
557.423520	40374.780596	31.602868
557.829451	40419.040020	31.607885
558.094075	40490.332977	31.612903
558.853891	40551.775045	31.617920
559.075874	40627.829275	31.622938
559.554020	40700.142060	31.627956
560.214944	40761.964169	31.632973
560.313324	40837.108504	31.637991
561.584516	40902.930659	31.643008
561.953828	40969.564888	31.648026
562.311021	41034.717766	31.653044
563.197172	41088.328223	31.658061
563.571277	41171.070508	31.663079
564.274936	41231.542430	31.668096
565.305161	41304.202034	31.673114
565.310941	41384.269314	31.678132
566.024694	41451.542870	31.683149
566.591975	41532.547129	31.688167
567.363589	41594.738883	31.693184
568.223677	41650.113563	31.698202
568.294908	41711.992080	31.703220
568.654399	41793.691561	31.708237
569.023217	41857.901583	31.713255
569.695890	41930.471200	31.718272
570.241816	42022.406627	31.723290
570.825878	42095.613411	31.728308
571.840849	42160.244951	31.733325
572.120573	42243.108669	31.738343
572.746599	42310.358821	31.743360
573.377269	42381.298771	31.748378
573.665391	42459.925629	31.753396
574.452896	42534.584268	31.758413
575.162246	42610.834546	31.763431
575.777437	42679.956696	31.768448
576.815099	42757.949618	31.773466
577.027920	42838.809814	31.778484
577.588785	42904.791197	31.783501
577.915806	42979.388786	31.788519
578.761203	43046.387564	31.793536
579.790792	43108.955387	31.798554
580.417588	43177.966992	31.803572
581.549302	43230.498192	31.808589
581.894624	43286.982515	31.813607
582.358268	43342.007885	31.818624
583.181645	43409.437810	31.823642
583.359554	43472.627390	31.828660
584.149015	43539.596154	31.833677
584.558926	43604.503167	31.838695
584.700246	43669.356900	31.843712
585.103688	43738.625320	31.848730
585.390803	43832.260480	31.853748
586.177753	43895.527708	31.858765
586.606946	43972.041393	31.863783
587.015527	44050.017379	31.868800
587.220969	44127.357934	31.873818
587.882101	44219.297886	31.878836
588.914014	44294.280017	31.883853
589.188599	44380.342865	31.888871
589.473944	44467.869260	31.893888
590.586338	44540.329140	31.898906
590.778856	44627.656929	31.903924
591.611189	44683.667260	31.908941
592.553674	44763.256636	31.913959
593.327161	44837.854258	31.918976
594.327034	44901.894842	31.923994
594.588231	44965.363048	31.929012
595.374132	45034.292131	31.934029
595.803403	45107.526911	31.939047
595.782233	45178.825176	31.944064
596.275542	45258.595042	31.949082
596.357761	45330.584046	31.954100
597.114269	45429.978123	31.959117
597.752202	45519.680298	31.964135
598.306476	45591.282922	31.969152
599.278288	45670.678726	31.974170
599.532381	45772.456168	31.979188
600.216027	45847.814650	31.984205
600.597861	45944.766359	31.989223
601.503583	46039.803890	31.994240
602.045072	46131.441489	31.999258
601.976642	46212.880605	32.004276
603.033339	46311.121508	32.009293
603.924996	46405.083353	32.014311
604.108836	46497.586968	32.019328
604.832244	46582.843805	32.024346
605.697244	46691.118254	32.029364
606.178485	46776.100208	32.034381
606.516887	46871.011453	32.039399
607.390212	46970.691212	32.044416
608.630664	47047.493982	32.049434
608.684893	47131.812341	32.054452
609.869094	47215.262407	32.059469
610.357131	47311.417370	32.064487
610.763163	47411.287152	32.069504
611.715921	47494.861938	32.074522
612.158454	47582.493741	32.079540
613.336124	47657.629474	32.084557
613.756051	47740.781798	32.089575
614.604897	47826.067752	32.094592
615.707558	47886.656464	32.099610
616.709264	47968.949535	32.104628
617.271620	48035.299298	32.109645
617.685249	48104.639014	32.114663
618.429276	48183.085185	32.119680
618.966552	48243.260011	32.124698
619.459421	48312.290567	32.129716
620.319967	48387.901569	32.134733
620.899882	48454.240426	32.139751
621.385988	48520.560271	32.144768
621.842440	48585.546312	32.149786
622.487218	48672.723448	32.154804
623.178675	48744.890133	32.159821
623.955188	48813.218827	32.164839
624.044349	48883.688664	32.169856
624.132884	48972.875894	32.174874
624.597804	49067.950947	32.179892
625.401595	49144.269083	32.184909
626.142946	49237.875093	32.189927
626.293011	49318.527258	32.194944
626.926425	49394.135565	32.199962
627.311430	49495.519839	32.204980
628.427949	49592.561555	32.209997
628.876463	49687.699253	32.215015
629.991649	49774.131081	32.220032
630.691982	49852.433453	32.225050
631.258441	49935.858567	32.230068
631.725685	50032.409712	32.235085
632.277430	50108.198557	32.240103
633.037864	50197.918486	32.245120
633.648432	50263.036385	32.250138
634.155106	50354.131691	32.255156
634.884360	50432.990659	32.260173
635.604684	50507.935281	32.265191
635.970908	50589.302438	32.270208
636.986796	50655.911725	32.275226
637.386144	50737.848835	32.280244
637.987965	50825.052373	32.285261
638.659712	50901.092987	32.290279
639.061432	50987.929214	32.295296
639.908618	51076.584071	32.300314
639.967959	51161.355264	32.305332
640.850598	51248.978618	32.310349
641.534822	51340.876760	32.315367
642.133714	51429.021542	32.320384
642.943842	51520.056473	32.325402
643.852311	51619.483157	32.330420
644.415840	51699.420114	32.335437
645.268001	51784.745327	32.340455
645.919791	51871.380004	32.345472
646.753347	51943.279456	32.350490
647.663767	52037.221804	32.355508
648.372642	52101.745391	32.360525
649.176043	52171.158662	32.365543
649.364204	52263.465290	32.370560
649.767604	52347.319453	32.375578
650.320547	52434.364632	32.380596
651.086480	52526.618158	32.385613
651.796211	52626.695604	32.390631
651.750046	52707.056432	32.395648
652.815184	52796.235947	32.400666
653.592858	52896.499397	32.405684
654.065522	52973.421242	32.410701
654.743661	53075.432959	32.415719
655.082329	53186.617049	32.420736
655.716570	53272.205917	32.425754
656.202495	53387.169831	32.430772
656.902624	53484.220980	32.435789
657.522802	53580.079200	32.440807
658.153039	53683.119114	32.445824
658.913603	53780.048045	32.450842
659.488534	53892.435367	32.455860
660.069781	53993.014880	32.460877
661.026360	54097.847804	32.465895
661.336949	54201.480238	32.470912
662.208657	54289.201286	32.475930
663.019269	54416.335886	32.480948
663.898778	54514.670294	32.485965
664.517366	54625.153006	32.490983
664.977077	54728.801515	32.496000
666.117566	54811.401060	32.501018
666.581326	54907.001012	32.506036
667.742406	55005.499876	32.511053
668.740234	55091.624242	32.516071
669.223050	55178.219429	32.521088
669.878116	55270.940198	32.526106
670.589264	55361.643039	32.531124
671.534374	55444.239613	32.536141
672.389067	55534.767918	32.541159
673.031104	55620.827006	32.546176
673.697269	55694.353790	32.551194
674.351438	55791.506120	32.556212
674.532628	55878.097341	32.561229
675.601391	55964.586594	32.566247
676.051337	56061.306439	32.571264
676.308306	56151.911023	32.576282
677.082223	56224.423718	32.581300
677.626779	56325.292942	32.586317
678.442768	56402.291622	32.591335
678.911793	56493.658858	32.596352
679.649817	56562.122372	32.601370
680.023483	56655.768067	32.606388
680.414257	56761.447912	32.611405
681.277213	56859.392414	32.616423
681.539818	56958.769739	32.621440
682.261709	57052.979016	32.626458
682.743331	57167.877334	32.631476
683.325364	57259.880254	32.636493
684.317855	57370.101794	32.641511
684.697071	57492.992963	32.646528
685.450983	57592.039582	32.651546
686.123622	57705.007551	32.656564
686.426310	57816.217463	32.661581
687.309581	57926.516999	32.666599
687.860792	58050.034041	32.671616
688.539911	58163.932411	32.676634
689.206840	58277.726025	32.681652
689.927763	58396.042030	32.686669
690.608235	58508.545667	32.691687
691.379448	58632.194279	32.696704
692.014401	58743.847379	32.701722
692.865216	58856.286932	32.706740
693.779799	58986.308946	32.711757
694.500292	59099.864595	32.716775
695.519547	59206.483659	32.721792
696.577066	59309.754115	32.726810
697.441544	59408.418668	32.731828
698.653115	59515.980784	32.736845
699.558936	59600.231538	32.741863
700.187080	59708.320746	32.746880
701.034789	59809.359790	32.751898
701.640825	59900.663161	32.756916
702.353256	59996.379287	32.761933
703.426012	60077.596438	32.766951
704.258289	60152.230831	32.771968
704.993801	60236.379673	32.776986
705.112909	60333.655188	32.782004
705.730817	60436.308895	32.787021
706.636092	60514.882300	32.792039
707.575108	60618.425526	32.797056
707.902282	60709.589032	32.802074
708.884788	60783.929215	32.807092
708.982338	60898.337305	32.812109
709.670486	60990.535777	32.817127
710.717423	61089.646111	32.822144
711.147891	61192.821243	32.827162
711.983133	61298.906694	32.832180
712.052695	61413.600393	32.837197
712.869602	61508.712379	32.842215
713.647122	61614.973336	32.847232
714.019688	61729.328068	32.852250
714.569731	61839.716780	32.857268
715.029123	61956.750771	32.862285
715.757958	62068.078165	32.867303
716.466408	62190.273785	32.872320
717.814475	62297.569076	32.877338
718.613527	62420.743382	32.882356
719.685619	62513.390992	32.887373
720.519016	62608.890944	32.892391
721.137022	62719.342733	32.897408
721.795172	62825.041948	32.902426
722.661105	62936.458899	32.907444
723.096663	63035.502731	32.912461
723.795915	63134.844799	32.917479
724.626291	63232.553990	32.922496
725.536615	63336.969090	32.927514
726.354341	63418.937011	32.932532
726.880675	63526.873795	32.937549
727.784649	63624.591668	32.942567
728.410453	63713.665155	32.947584
729.136338	63808.095013	32.952602
729.754895	63914.084505	32.957620
730.159799	64018.276832	32.962637
730.587544	64109.489527	32.967655
731.168566	64231.509822	32.972672
732.042797	64337.806921	32.977690
732.905487	64449.422266	32.982708
732.740118	64560.133444	32.987725
733.634588	64690.087912	32.992743
734.261814	64804.759124	32.997760
734.670442	64939.213706	33.002778
735.342613	65061.729546	33.007796
735.780481	65192.097590	33.012813
737.025580	65313.085439	33.017831
737.564883	65465.675972	33.022848
738.124078	65592.777459	33.027866
739.345613	65724.024511	33.032884
740.022935	65856.873038	33.037901
740.632792	65981.724510	33.042919
741.227264	66124.443290	33.047936
741.911939	66247.286471	33.052954
743.279972	66389.879337	33.057972
744.125647	66527.375864	33.062989
744.839715	66655.690969	33.068007
745.638834	66794.050347	33.073024
746.262969	66911.723811	33.078042
747.071048	67026.586068	33.083060
747.554070	67169.185023	33.088077
748.409528	67304.554679	33.093095
749.205682	67442.950461	33.098112
749.629009	67593.736145	33.103130
750.679093	67710.932864	33.108148
751.364960	67864.882297	33.113165
752.524868	67990.495780	33.118183
753.873024	68112.083482	33.123200
754.168877	68244.144116	33.128218
754.836063	68368.905582	33.133236
755.631420	68501.353177	33.138253
756.238109	68642.323303	33.143271
757.406239	68762.104778	33.148288
758.101544	68897.479560	33.153306
758.554328	69019.460613	33.158324
759.289540	69156.385727	33.163341
760.715706	69288.051308	33.168359
761.256674	69413.908274	33.173376
761.570563	69536.775087	33.178394
763.506303	69659.722529	33.183412
764.328932	69779.762836	33.188429
765.172890	69878.708625	33.193447
766.151170	69999.110144	33.198464
766.823915	70119.859959	33.203482
767.531829	70228.990133	33.208500
768.220879	70346.355983	33.213517
768.586683	70467.341816	33.218535
769.229824	70576.079823	33.223552
769.945308	70698.754283	33.228570
770.881309	70821.412006	33.233588
771.527828	70944.276306	33.238605
772.111042	71071.084549	33.243623
772.871628	71211.331898	33.248640
773.328537	71329.702579	33.253658
774.323012	71457.216599	33.258676
775.127838	71585.413960	33.263693
775.631653	71709.482302	33.268711
776.493782	71835.958176	33.273728
776.683575	71961.824989	33.278746
777.837926	72079.490289	33.283764
778.368425	72204.967148	33.288781
779.173892	72330.626970	33.293799
780.107637	72456.310609	33.298816
780.920362	72587.813383	33.303834
781.792926	72702.853905	33.308852
782.780147	72847.374382	33.313869
783.487396	72968.526659	33.318887
784.438519	73090.195807	33.323904
785.071437	73220.941720	33.328922
785.846780	73337.494019	33.333940
787.053074	73460.217082	33.338957
787.686208	73592.255205	33.343975
788.561828	73705.770285	33.348992
789.003073	73830.164732	33.354010
789.825804	73961.807037	33.359028
790.386805	74094.182643	33.364045
791.526721	74231.155669	33.369063
792.625007	74350.284451	33.374080
793.125549	74485.979761	33.379098
793.551197	74604.379943	33.384116
794.746078	74744.970697	33.389133
795.877783	74872.798486	33.394151
796.699890	75005.927028	33.399168
797.092549	75127.371002	33.404186
797.785366	75262.963524	33.409204
798.940476	75398.796757	33.414221
799.518898	75530.476263	33.419239
800.439323	75658.748297	33.424256
801.000854	75802.245729	33.429274
802.646950	75912.362868	33.434292
803.346830	76046.270524	33.439309
804.578527	76164.052788	33.444327
805.667080	76286.374888	33.449344
806.166478	76404.481743	33.454362
807.052255	76524.410102	33.459380
808.326374	76633.415959	33.464397
808.562974	76751.112715	33.469415
809.600161	76876.937691	33.474432
810.205944	76997.680132	33.479450
810.888067	77125.690202	33.484468
811.222444	77258.571457	33.489485
811.909169	77382.983563	33.494503
812.783379	77506.865765	33.499520
813.266457	77641.565253	33.504538
814.251581	77779.326065	33.509556
815.294407	77913.017693	33.514573
816.233581	78029.941161	33.519591
817.361690	78183.499268	33.524608
818.019345	78302.874112	33.529626
818.898972	78408.747167	33.534644
819.651471	78549.283553	33.539661
819.816798	78673.782689	33.544679
820.801932	78814.800994	33.549696
821.761598	78953.224789	33.554714
822.832053	79075.027707	33.559732
823.439496	79219.868067	33.564749
823.923260	79364.805692	33.569767
824.873866	79486.130958	33.574784
825.701007	79635.763898	33.579802
825.865142	79774.425357	33.584820
826.699777	79916.481210	33.589837
827.454705	80072.555563	33.594855
828.221986	80214.649733	33.599872
828.653437	80359.691001	33.604890
829.807325	80518.738818	33.609908
830.600596	80668.358950	33.614925
831.173093	80802.563068	33.619943
832.105179	80945.128048	33.624960
833.090384	81103.961161	33.629978
834.154767	81235.088262	33.634996
835.085434	81372.538670	33.640013
836.164538	81510.079271	33.645031
837.277873	81641.611833	33.650048
837.828611	81782.214481	33.655066
838.567933	81919.143135	33.660084
839.776649	82053.509010	33.665101
840.594628	82191.425826	33.670119
841.507085	82339.455866	33.675136
841.946784	82471.825653	33.680154
843.008422	82610.014760	33.685172
843.503300	82766.675769	33.690189
844.130639	82920.304714	33.695207
845.341437	83054.790050	33.700224
846.221358	83212.807630	33.705242
846.717866	83349.221962	33.710260
847.136874	83518.660858	33.715277
848.346781	83670.965030	33.720295
849.380892	83821.755591	33.725312
849.862369	83976.554493	33.730330
850.692168	84146.430005	33.735348
851.681063	84301.305483	33.740365
852.640353	84465.297236	33.745383
853.554038	84608.698056	33.750400
854.760018	84749.558788	33.755418
856.046048	84907.824699	33.760436
856.976656	85054.635626	33.765453
857.730853	85195.953295	33.770471
858.653195	85343.520320	33.775488
859.453946	85495.518222	33.780506
860.436788	85635.927720	33.785524
861.243261	85797.309529	33.790541
861.451664	85948.667956	33.795559
862.450003	86098.726434	33.800576
863.562218	86253.822448	33.805594
864.352973	86405.056065	33.810612
865.313731	86566.310192	33.815629
866.009604	86714.935705	33.820647
866.947317	86863.825946	33.825664
868.255670	87019.615999	33.830682
869.155849	87178.979852	33.835700
870.018375	87326.537736	33.840717
870.690388	87480.885724	33.845735
871.927427	87631.015916	33.850752
872.754945	87795.084642	33.855770
873.392938	87938.064360	33.860788
873.768286	88097.786891	33.865805
874.447664	88261.528996	33.870823
875.256548	88407.995215	33.875840
875.656670	88587.351847	33.880858
876.895236	88757.041749	33.885876
877.559353	88917.633374	33.890893
878.398990	89111.013523	33.895911
879.504778	89278.115684	33.900928
880.124423	89446.780043	33.905946
881.054765	89603.130598	33.910964
882.030771	89774.965749	33.915981
882.657345	89948.783588	33.920999
883.884245	90128.382443	33.926016
884.440187	90306.846781	33.931034
885.300876	90469.757921	33.936052
886.136196	90635.034820	33.941069
886.726835	90831.900058	33.946087
887.631690	91006.888400	33.951104
888.430004	91175.579834	33.956122
889.257474	91351.577045	33.961140
889.852034	91527.930433	33.966157
890.779916	91711.919310	33.971175
891.939423	91893.029802	33.976192
892.765974	92054.495476	33.981210
893.593619	92239.087185	33.986228
894.568788	92424.991324	33.991245
895.305703	92616.935957	33.996263
896.480222	92784.576639	34.001280
897.512679	92963.494741	34.006298
898.198272	93139.408225	34.011316
899.187251	93324.323372	34.016333
899.886011	93508.446086	34.021351
901.135161	93696.333748	34.026368
902.012773	93871.606926	34.031386
902.614245	94062.591718	34.036404
904.236886	94234.453323	34.041421
904.748138	94426.797671	34.046439
906.084159	94606.614515	34.051456
907.034894	94790.781292	34.056474
908.002619	94969.262824	34.061492
909.306533	95146.209055	34.066509
909.813182	95319.977859	34.071527
910.804020	95497.870786	34.076544
911.447977	95686.772511	34.081562
912.721107	95867.507817	34.086580
914.093188	96039.309556	34.091597
914.770140	96223.551295	34.096615
915.560595	96390.033242	34.101632
916.392283	96573.758327	34.106650
917.485569	96761.131917	34.111668
918.771370	96930.688014	34.116685
918.965388	97118.928071	34.121703
920.248763	97288.892143	34.126720
921.192035	97469.997491	34.131738
921.970821	97653.011364	34.136756
923.137036	97842.305447	34.141773
923.642870	98023.727600	34.146791
925.236282	98177.751403	34.151808
926.212538	98374.132798	34.156826
926.921809	98552.885475	34.161844
928.290541	98713.602883	34.166861
928.607988	98907.736006	34.171879
929.874626	99083.298537	34.176896
930.478402	99256.471180	34.181914
931.734624	99440.381567	34.186932
933.128457	99614.382155	34.191949
934.663449	99774.547145	34.196967
935.564874	99939.160617	34.201984
936.688702	100102.535604	34.207002
937.589289	100257.851440	34.212020
938.563159	100417.233180	34.217037
939.330956	100588.412685	34.222055
940.508765	100744.951918	34.227072
941.483023	100914.523147	34.232090
942.093450	101071.360661	34.237108
943.112586	101235.671913	34.242125
944.084573	101393.952178	34.247143
945.092381	101554.272461	34.252160
946.138078	101706.603929	34.257178
946.917017	101864.013636	34.262196
948.040665	102024.102489	34.267213
948.572173	102201.181912	34.272231
949.228372	102366.117524	34.277248
950.186134	102547.136681	34.282266
950.578740	102711.143006	34.287284
951.412340	102870.632908	34.292301
952.049708	103045.111128	34.297319
952.459639	103220.495498	34.302336
953.351222	103399.632135	34.307354
954.190524	103596.469149	34.312372
955.236586	103760.140004	34.317389
955.896639	103956.825742	34.322407
957.014294	104137.253497	34.327424
957.499075	104341.151284	34.332442
958.441497	104541.650903	34.337460
959.677884	104726.463784	34.342477
960.539911	104925.105399	34.347495
961.365376	105127.091519	34.352512
962.645301	105333.892501	34.357530
963.463600	105525.580681	34.362548
964.630613	105721.075291	34.367565
965.910758	105932.801039	34.372583
966.715364	106116.225988	34.377600
968.148357	106311.617773	34.382618
968.831196	106515.911446	34.387636
970.011854	106706.281974	34.392653
970.894448	106912.686087	34.397671
971.625071	107113.670990	34.402688
972.860504	107301.225161	34.407706
973.716472	107497.620224	34.412724
975.043852	107701.677351	34.417741
975.815905	107898.405870	34.422759
976.919324	108102.807027	34.427776
977.995855	108300.868787	34.432794
979.186296	108496.025464	34.437812
980.387830	108704.873332	34.442829
981.204940	108901.652491	34.447847
981.833699	109102.466608	34.452864
983.003745	109301.698286	34.457882
983.664715	109508.437798	34.462900
984.703949	109705.084863	34.467917
985.795157	109915.416997	34.472935
986.665185	110121.037412	34.477952
987.662969	110332.224206	34.482970
988.507597	110538.561319	34.487988
989.410482	110749.222381	34.493005
990.130458	110959.915280	34.498023
991.303140	111177.400504	34.503040
992.663261	111385.052318	34.508058
993.458536	111610.773497	34.513076
994.641190	111810.464958	34.518093
995.806396	112024.652074	34.523111
996.797207	112233.106028	34.528128
998.388262	112429.200411	34.533146
998.756499	112645.766103	34.538164
1000.097593	112865.263795	34.543181
1001.116718	113059.987671	34.548199
1002.028783	113273.795649	34.553216
1003.216833	113471.116786	34.558234
1003.997573	113686.862505	34.563252
1005.019799	113902.608047	34.568269
1005.971309	114102.747065	34.573287
1006.688076	114311.135331	34.578304
1008.317998	114529.306424	34.583322
1009.537746	114721.044491	34.588340
1011.080050	114919.799688	34.593357
1012.350112	115116.865646	34.598375
1013.285560	115301.053455	34.603392
1014.293106	115492.603832	34.608410
1015.793800	115696.223596	34.613428
1016.516269	115867.806728	34.618445
1016.859073	116066.666764	34.623463
1017.528933	116275.039442	34.628480
1019.061250	116456.475790	34.633498
1019.845324	116631.360093	34.638516
1020.475918	116806.726919	34.643533
1021.418658	117013.412989	34.648551
1022.327846	117208.513427	34.653568
1023.475354	117387.510715	34.658586
1023.754323	117601.190293	34.663604
1025.145711	117803.981799	34.668621
1026.329530	118001.183563	34.673639
1027.474548	118206.793337	34.678656
1028.537668	118400.001388	34.683674
1029.354081	118599.396530	34.688692
1030.337130	118801.033538	34.693709
1030.903031	119012.142267	34.698727
1031.995748	119218.806932	34.703744
1032.776056	119438.030526	34.708762
1033.398283	119664.288776	34.713780
1034.892082	119885.640705	34.718797
1035.729535	120110.194383	34.723815
1036.825262	120347.428835	34.728832
1037.708790	120576.426045	34.733850
1038.720804	120800.639488	34.738868
1039.712771	121029.153536	34.743885
1040.938030	121262.788122	34.748903
1042.064116	121486.430482	34.753920
1043.263376	121712.698167	34.758938
1044.082126	121935.013499	34.763956
1045.427481	122170.130780	34.768973
1046.425170	122395.588013	34.773991
1047.379706	122638.364019	34.779008
1048.781524	122871.209312	34.784026
1049.530129	123114.618829	34.789044
1050.812738	123348.412639	34.794061
1051.787114	123568.560338	34.799079
1052.999461	123810.682482	34.804096
1054.019651	124030.864069	34.809114
1055.117834	124275.594057	34.814132
1056.525396	124487.490510	34.819149
1057.547255	124726.052487	34.824167
1058.641349	124975.655279	34.829184
1059.731318	125189.383359	34.834202
1060.636000	125415.373149	34.839220
1061.790924	125660.497977	34.844237
1062.979401	125883.212755	34.849255
1063.313188	126137.044208	34.854272
1064.591775	126364.120008	34.859290
1065.831215	126603.890310	34.864308
1067.099070	126841.642691	34.869325
1068.117739	127069.425723	34.874343
1069.137100	127295.207864	34.879360
1070.588586	127531.870720	34.884378
1071.365943	127760.243740	34.889396
1072.583896	127995.896792	34.894413
1073.943433	128223.746243	34.899431
1074.939599	128456.321563	34.904448
1076.559645	128694.473844	34.909466
1077.142644	128931.366930	34.914484
1078.103889	129156.120385	34.919501
1079.219497	129393.524807	34.924519
1080.045430	129623.513347	34.929536
1081.361266	129850.013146	34.934554
1082.259472	130096.470768	34.939572
1082.879279	130338.083672	34.944589
1084.139148	130576.930976	34.949607
1084.966635	130825.725617	34.954624
1086.235368	131064.258298	34.959642
1087.029022	131322.429662	34.964660
1088.494069	131543.720122	34.969677
1090.085009	131770.492646	34.974695
1090.845783	132001.688288	34.979712
1091.742494	132208.360551	34.984730
1092.782713	132463.420302	34.989748
1093.708205	132680.295123	34.994765
1095.154990	132903.106583	34.999783
1095.903800	133143.160539	35.004800
1097.198378	133371.666725	35.009818
1098.542507	133610.294902	35.014836
1098.901264	133849.987558	35.019853
1100.274920	134073.047440	35.024871
1101.385229	134319.718496	35.029888
1102.631151	134545.908561	35.034906
1103.702285	134782.917174	35.039924
1105.160954	135025.048477	35.044941
1106.475651	135261.576699	35.049959
1107.745923	135491.166846	35.054976
1109.023791	135723.394250	35.059994
1109.928400	135963.405488	35.065012
1111.094114	136195.857616	35.070029
1112.145489	136426.289177	35.075047
1112.649410	136672.609158	35.080064
1114.127423	136919.454794	35.085082
1114.972483	137153.551379	35.090100
1115.878210	137396.666342	35.095117
1117.334404	137655.907507	35.100135
1117.837378	137916.943542	35.105152
1119.114860	138166.278507	35.110170
1119.962627	138424.586505	35.115188
1120.875747	138686.904800	35.120205
1122.510896	138947.850794	35.125223
1123.608450	139207.213984	35.130240
1125.020341	139462.317942	35.135258
1126.283283	139728.884775	35.140276
1127.046632	139978.178672	35.145293
1128.274169	140244.375065	35.150311
1128.997652	140508.399868	35.155328
1129.860451	140764.428473	35.160346
1131.492183	141042.432222	35.165364
1132.528487	141302.202016	35.170381
1134.317011	141575.809828	35.175399
1135.210409	141833.629249	35.180416
1136.527168	142085.611438	35.185434
1137.724203	142352.298513	35.190452
1138.870022	142613.404253	35.195469
1140.237169	142849.964912	35.200487
1140.936094	143141.986294	35.205504
1142.383343	143393.411268	35.210522
1143.931862	143655.168502	35.215540
1144.738477	143919.053681	35.220557
1146.183253	144163.282152	35.225575
1147.008255	144437.236552	35.230592
1148.354608	144695.382951	35.235610
1149.257932	144961.517204	35.240628
1150.192081	145224.807861	35.245645
1151.633428	145482.830237	35.250663
1152.591385	145753.120819	35.255680
1153.530536	146017.862209	35.260698
1154.390425	146285.370496	35.265716
1155.212428	146568.928996	35.270733
1156.142075	146835.973375	35.275751
1157.173212	147139.602036	35.280768
1158.386386	147419.057286	35.285786
1159.700901	147706.018282	35.290804
1161.016693	147994.274907	35.295821
1162.366677	148272.268463	35.300839
1163.195709	148563.247825	35.305856
1164.322919	148836.171599	35.310874
1165.583241	149117.699398	35.315892
1166.821924	149364.242280	35.320909
1168.186796	149626.834665	35.325927
1169.394559	149898.814588	35.330944
1170.570557	150163.116086	35.335962
1172.094152	150407.767291	35.340980
1173.176675	150683.527773	35.345997
1174.719025	150943.259307	35.351015
1175.873442	151199.442041	35.356032
1176.884065	151470.286558	35.361050
1178.539294	151729.662516	35.366068
1179.855231	151997.327721	35.371085
1181.124738	152244.912069	35.376103
1182.584415	152498.377144	35.381120
1183.937416	152752.115206	35.386138
1185.122111	153002.382082	35.391156
1186.230888	153254.185190	35.396173
1187.279039	153502.106060	35.401191
1188.438609	153757.950254	35.406208
1189.854185	154018.903593	35.411226
1190.867676	154285.962686	35.416244
1191.599408	154544.698631	35.421261
1192.871467	154806.010818	35.426279
1193.971087	155084.477043	35.431296
1195.030328	155339.384357	35.436314
1196.044592	155617.462617	35.441332
1197.321186	155890.844340	35.446349
1198.595427	156164.355222	35.451367
1199.496676	156450.627018	35.456384
1200.463594	156719.676753	35.461402
1201.522642	156998.734217	35.466420
1202.937902	157290.737008	35.471437
1204.235949	157567.704091	35.476455
1206.040436	157845.325267	35.481472
1207.503837	158117.600761	35.486490
1209.289248	158384.497120	35.491508
1210.280500	158665.429609	35.496525
1211.506826	158919.444614	35.501543
1212.397342	159186.722389	35.506560
1213.566454	159468.202012	35.511578
1215.102297	159738.738660	35.516596
1216.235107	160018.934174	35.521613
1217.513704	160300.490337	35.526631
1218.336206	160570.046609	35.531648
1219.450116	160837.742452	35.536666
1220.931856	161110.606064	35.541684
1221.634896	161396.806475	35.546701
1222.975182	161681.191038	35.551719
1223.819751	161977.064542	35.556736
1225.008825	162268.303451	35.561754
1226.166480	162558.268242	35.566772
1227.361362	162865.203800	35.571789
1228.236735	163162.501601	35.576807
1229.708193	163460.007619	35.581824
1231.087367	163753.889805	35.586842
1232.298149	164053.434923	35.591860
1233.215406	164363.459507	35.596877
1235.077528	164648.970787	35.601895
1236.026238	164944.353291	35.606912
1237.378629	165242.069152	35.611930
1238.807627	165547.805676	35.616948
1239.727846	165857.751849	35.621965
1240.881286	166147.183738	35.626983
1241.851964	166472.871509	35.632000
1242.998774	166760.646501	35.637018
1244.203676	167075.210898	35.642036
1244.962078	167382.644420	35.647053
1246.828962	167694.084256	35.652071
1247.921916	167992.965761	35.657088
1249.009034	168299.057256	35.662106
1250.520055	168589.715189	35.667124
1250.999425	168893.132339	35.672141
1252.498180	169199.555470	35.677159
1253.413935	169508.259395	35.682176
1254.365555	169813.343223	35.687194
1255.988163	170122.835627	35.692212
1256.963650	170443.983939	35.697229
1258.412805	170760.640562	35.702247
1259.540714	171088.442745	35.707264
1260.476187	171413.880784	35.712282
1262.235136	171737.599064	35.717300
1263.163886	172071.646269	35.722317
1264.600880	172387.301035	35.727335
1266.344486	172710.876429	35.732352
1267.658720	173034.195021	35.737370
1269.374332	173342.615258	35.742388
1270.595353	173671.740203	35.747405
1272.152889	173988.083893	35.752423
1273.327968	174303.388802	35.757440
1274.667928	174630.229314	35.762458
1276.042897	174952.231331	35.767476
1276.755303	175264.547972	35.772493
1277.869693	175589.401862	35.777511
1279.343405	175928.627721	35.782528
1280.472866	176254.511556	35.787546
1281.873899	176583.855389	35.792564
1283.066124	176929.378540	35.797581
1284.245302	177264.702874	35.802599
1286.009242	177599.399980	35.807616
1287.335849	177927.737215	35.812634
1289.454989	178245.996032	35.817652
1290.585681	178569.141148	35.822669
1291.849764	178892.279044	35.827687
1292.832051	179216.721986	35.832704
1294.183429	179542.514863	35.837722
1295.708845	179871.035183	35.842740
1296.780663	180201.028581	35.847757
1298.130139	180538.847131	35.852775
1299.608263	180866.899437	35.857792
1300.436752	181203.310752	35.862810
1302.164776	181520.106433	35.867828
1303.317207	181867.637509	35.872845
1304.634672	182201.563167	35.877863
1305.991656	182531.905265	35.882880
1307.140980	182866.992546	35.887898
1308.660033	183200.269411	35.892916
1309.729144	183539.029606	35.897933
1311.209249	183877.939915	35.902951
1312.489707	184202.733141	35.907968
1314.007112	184535.422136	35.912986
1315.624454	184853.309702	35.918004
1317.547459	185194.744587	35.923021
1318.899640	185516.360737	35.928039
1320.358349	185825.649067	35.933056
1321.579535	186153.548226	35.938074
1323.060295	186465.730552	35.943092
1324.113526	186788.850553	35.948109
1325.365067	187113.462906	35.953127
1326.362541	187447.766004	35.958144
1327.572060	187768.543049	35.963162
1328.870939	188094.930388	35.968180
1330.015566	188427.146023	35.973197
1330.916676	188757.677474	35.978215
1332.592989	189092.449541	35.983232
1333.726065	189429.712350	35.988250
1335.229558	189750.388654	35.993268
1336.667424	190081.372328	35.998285
1337.900478	190387.981203	36.003303
1338.931084	190717.182408	36.008320
1340.664206	191037.992976	36.013338
1341.771407	191373.075303	36.018356
1342.524489	191703.876547	36.023373
1343.706304	192038.709152	36.028391
1345.140050	192364.755631	36.033408
1346.776401	192716.311715	36.038426
1348.163025	193035.641563	36.043444
1349.371043	193382.194417	36.048461
1351.068633	193702.035031	36.053479
1352.575191	194032.991362	36.058496
1353.714714	194369.354571	36.063514
1354.900831	194710.447121	36.068532
1356.022674	195061.365358	36.073549
1357.210081	195401.179308	36.078567
1358.766516	195752.969151	36.083584
1359.689874	196117.014717	36.088602
1361.116838	196466.138537	36.093620
1362.731168	196805.229456	36.098637
1363.891718	197186.190240	36.103655
1365.290728	197532.899690	36.108672
1366.589583	197906.808635	36.113690
1367.982946	198279.891619	36.118708
1369.296386	198636.244341	36.123725
1370.491900	199003.689135	36.128743
1371.952462	199375.269151	36.133760
1373.196330	199755.342457	36.138778
1374.570748	200124.744477	36.143796
1375.787035	200508.965480	36.148813
1376.760694	200894.269780	36.153831
1378.186237	201284.592845	36.158848
1379.794873	201668.412834	36.163866
1381.077178	202057.684738	36.168884
1382.567205	202454.453492	36.173901
1383.727752	202836.982669	36.178919
1385.710997	203227.846728	36.183936
1386.768136	203631.486181	36.188954
1388.003242	204019.545138	36.193972
1389.366135	204412.638395	36.198989
1390.719504	204818.978114	36.204007
1392.574758	205207.296599	36.209024
1393.650160	205605.916075	36.214042
1395.126710	206020.025324	36.219060
1396.677172	206415.840891	36.224077
1398.242820	206817.534811	36.229095
1399.521963	207210.771017	36.234112
1400.937212	207616.303141	36.239130
1402.962635	208012.620024	36.244148
1404.596559	208405.918075	36.249165
1406.028148	208796.369176	36.254183
1407.362840	209182.863881	36.259200
1408.779374	209582.031857	36.264218
1410.233412	209961.082562	36.269236
1411.689093	210362.546243	36.274253
1412.736291	210759.000211	36.279271
1414.240957	211149.780865	36.284288
1415.561979	211548.428280	36.289306
1417.266472	211941.935147	36.294324
1418.288649	212340.711856	36.299341
1419.579496	212739.065171	36.304359
1421.357955	213137.416073	36.309376
1422.496857	213542.096482	36.314394
1424.266419	213939.868448	36.319412
1425.548562	214337.519489	36.324429
1426.507533	214745.257367	36.329447
1427.699039	215142.012701	36.334464
1429.333596	215537.147466	36.339482
1430.846800	215925.116614	36.344500
1431.929929	216323.114079	36.349517
1433.070403	216711.198861	36.354535
1434.722537	217114.058309	36.359552
1436.048437	217514.687550	36.364570
1437.394282	217919.353420	36.369588
1439.090191	218327.620511	36.374605
1440.411705	218718.045648	36.379623
1441.691079	219119.959171	36.384640
1443.371379	219525.567089	36.389658
1445.105148	219959.461371	36.394676
1446.478441	220408.478184	36.399693
1447.570991	220819.928338	36.404711
1449.023117	221222.888522	36.409728
1450.590287	221634.263614	36.414746
1451.890791	222047.487636	36.419764
1453.543120	222465.455584	36.424781
1455.181912	222872.963074	36.429799
1456.805442	223277.452148	36.434816
1458.119041	223691.975691	36.439834
1460.247710	224110.023770	36.444852
1461.922199	224520.020609	36.449869
1463.590513	224936.445987	36.454887
1465.374626	225327.657556	36.459904
1466.483582	225742.908194	36.464922
1467.796202	226146.366690	36.469940
1469.032069	226555.604956	36.474957
1470.515574	226969.121721	36.479975
1471.877265	227398.992107	36.484992
1473.055757	227820.639250	36.490010
1474.548841	228228.164298	36.495028
1476.203738	228650.777033	36.500045
1477.584795	229082.859829	36.505063
1479.566940	229497.420295	36.510080
1480.921231	229928.849916	36.515098
1482.332769	230359.077674	36.520116
1483.374965	230774.584650	36.525133
1485.014203	231212.397702	36.530151
1486.374193	231644.136655	36.535168
1487.757896	232074.475981	36.540186
1489.095118	232518.642330	36.545204
1490.750638	232950.869892	36.550221
1492.242703	233409.847536	36.555239
1493.603938	233841.186418	36.560256
1495.067437	234280.714216	36.565274
1496.106137	234730.499246	36.570292
1498.072961	235181.326275	36.575309
1499.189485	235626.528776	36.580327
1500.666780	236087.269437	36.585344
1502.053711	236545.917965	36.590362
1503.937551	236998.770395	36.595380
1505.707405	237455.910298	36.600397
1507.333080	237908.502879	36.605415
1508.669408	238352.025120	36.610432
1510.512636	238813.703300	36.615450
1511.768604	239258.307856	36.620468
1513.374878	239715.404205	36.625485
1514.870126	240174.298090	36.630503
1516.465964	240611.533887	36.635520
1518.149592	241072.532513	36.640538
1519.874690	241531.137515	36.645556
1522.059119	241963.020791	36.650573
1522.936298	242405.637164	36.655591
1525.111048	242843.747319	36.660608
1526.601898	243285.095653	36.665626
1528.116095	243719.404499	36.670644
1529.674825	244149.566183	36.675661
1531.076873	244561.718698	36.680679
1532.845945	244971.220267	36.685696
1533.872356	245396.010364	36.690714
1535.182299	245818.823755	36.695732
1536.678439	246234.773761	36.700749
1537.959981	246668.922717	36.705767
1539.500078	247094.062495	36.710784
1540.551020	247531.197486	36.715802
1541.866175	247992.269745	36.720820
1543.483122	248422.479228	36.725837
1544.742641	248882.469604	36.730855
1546.484831	249330.060544	36.735872
1548.151119	249775.683138	36.740890
1549.195660	250250.469847	36.745908
1550.781230	250701.822511	36.750925
1552.123725	251170.718466	36.755943
1554.004795	251640.262759	36.760960
1555.542943	252101.201676	36.765978
1556.900683	252573.221159	36.770996
1559.130206	253030.820688	36.776013
1560.760034	253511.052151	36.781031
1562.253286	253971.593700	36.786048
1563.561154	254440.346014	36.791066
1565.269907	254928.745407	36.796084
1567.219728	255387.866257	36.801101
1568.466491	255875.758235	36.806119
1569.647712	256350.883476	36.811136
1571.299001	256824.889866	36.816154
1572.843165	257324.546048	36.821172
1574.311257	257808.083906	36.826189
1575.700184	258304.387445	36.831207
1577.152105	258802.281145	36.836224
1579.453641	259294.496860	36.841242
1580.990615	259771.495213	36.846260
1583.237399	260265.041075	36.851277
1584.667223	260760.525394	36.856295
1586.000939	261249.293693	36.861312
1588.249914	261739.054098	36.866330
1589.401029	262216.116110	36.871348
1591.229429	262707.469963	36.876365
1592.485850	263195.869676	36.881383
1594.373133	263692.446628	36.886400
1595.923979	264182.093012	36.891418
1597.072544	264690.273737	36.896436
1599.026964	265170.809536	36.901453
1600.402173	265683.220094	36.906471
1601.766823	266173.886923	36.911488
1603.350906	266675.364393	36.916506
1604.855233	267189.911892	36.921524
1607.067793	267692.275620	36.926541
1608.114469	268201.944157	36.931559
1609.598508	268719.618247	36.936576
1611.540068	269224.895832	36.941594
1612.656736	269741.130688	36.946612
1614.573944	270259.620760	36.951629
1616.334701	270763.148252	36.956647
1617.850226	271280.179152	36.961664
1619.295136	271796.687552	36.966682
1620.449705	272332.168287	36.971700
1622.036575	272839.760761	36.976717
1623.296856	273373.368029	36.981735
1625.270425	273908.965164	36.986752
1627.578361	274424.692082	36.991770
1629.379094	274948.249609	36.996788
1631.009340	275459.209201	37.001805
1632.852271	275984.078783	37.006823
1634.817661	276501.890630	37.011840
1636.544210	277004.524760	37.016858
1637.781233	277489.329931	37.021876
1639.669337	277972.527980	37.026893
1641.430717	278465.729068	37.031911
1642.987444	278946.896783	37.036928
1644.429762	279445.178038	37.041946
1645.486721	279946.798613	37.046964
1646.693611	280441.001257	37.051981
1648.584133	280957.291318	37.056999
1650.187733	281460.291361	37.062016
1651.375380	281981.648120	37.067034
1653.235255	282498.066210	37.072052
1655.114437	283011.660098	37.077069
1656.662862	283549.032299	37.082087
1657.824856	284058.169241	37.087104
1659.727942	284576.377796	37.092122
1661.199784	285125.163088	37.097140
1662.649598	285658.379171	37.102157
1664.310723	286197.680371	37.107175
1665.984480	286742.007113	37.112192
1667.735096	287266.150801	37.117210
1669.308919	287828.880636	37.122228
1671.112051	288368.912907	37.127245
1672.878295	288932.318065	37.132263
1674.598838	289486.939916	37.137280
1676.298014	290033.434922	37.142298
1677.525791	290603.399454	37.147316
1679.279300	291155.011967	37.152333
1680.493857	291729.139617	37.157351
1682.002465	292309.032904	37.162368
1684.013199	292875.124701	37.167386
1685.671762	293454.378467	37.172404
1687.810741	294038.020665	37.177421
1689.470560	294618.411770	37.182439
1690.765765	295203.406766	37.187456
1692.273883	295775.029017	37.192474
1694.094237	296374.333060	37.197492
1695.839003	296967.068039	37.202509
1697.631436	297555.702785	37.207527
1699.540127	298135.730380	37.212544
1701.866573	298721.527705	37.217562
1703.800288	299307.158040	37.222580
1705.326785	299880.051452	37.227597
1707.436038	300460.160319	37.232615
1709.243109	301042.500016	37.237632
1711.100909	301625.539145	37.242650
1712.893140	302203.099728	37.247668
1714.504077	302759.682838	37.252685
1716.469014	303358.974034	37.257703
1717.787012	303948.133015	37.262720
1719.640354	304509.745473	37.267738
1721.037907	305102.922265	37.272756
1722.621831	305686.007267	37.277773
1724.374691	306264.666999	37.282791
1726.073120	306851.509717	37.287808
1728.000256	307445.472637	37.292826
1729.779442	308032.243365	37.297844
1731.695048	308615.101985	37.302861
1733.345618	309204.755682	37.307879
1735.083116	309790.835497	37.312896
1736.864671	310368.929684	37.317914
1738.916453	310953.578053	37.322932
1740.988406	311524.403853	37.327949
1743.193223	312111.685106	37.332967
1744.832759	312675.234838	37.337984
1746.845271	313246.286633	37.343002
1748.241886	313824.800258	37.348020
1749.642328	314387.945313	37.353037
1750.891623	314970.461494	37.358055
1752.701313	315534.444698	37.363072
1754.712114	316084.373087	37.368090
1755.888841	316659.447659	37.373108
1757.410128	317215.644360	37.378125
1758.955539	317794.178813	37.383143
1760.162327	318368.041355	37.388160
1762.085122	318933.731622	37.393178
1763.993327	319530.398670	37.398196
1765.635664	320105.165460	37.403213
1767.517521	320695.834197	37.408231
1769.181697	321284.553149	37.413248
1771.336676	321864.781346	37.418266
1772.734131	322468.464225	37.423284
1774.228649	323054.250152	37.428301
1776.660737	323642.212151	37.433319
1778.245403	324252.195461	37.438336
1780.127251	324855.217734	37.443354
1781.669293	325458.163399	37.448372
1783.140614	326072.286586	37.453389
1785.527189	326681.555644	37.458407
1786.964451	327288.969529	37.463424
1788.658820	327904.637283	37.468442
1790.535055	328531.846195	37.473460
1791.999810	329164.270368	37.478477
1793.859420	329784.487004	37.483495
1795.387621	330433.592815	37.488512
1797.233151	331064.131283	37.493530
1798.763841	331703.524352	37.498548
1800.601374	332340.854094	37.503565
1802.474878	332999.495925	37.508583
1804.381693	333637.916698	37.513600
1806.299242	334288.183912	37.518618
1808.259722	334948.057790	37.523636
1809.703847	335599.250794	37.528653
1811.475523	336260.028509	37.533671
1813.364451	336927.252044	37.538688
1815.346002	337588.562679	37.543706
1816.979450	338250.836344	37.548724
1818.370821	338911.669320	37.553741
1820.702261	339589.980729	37.558759
1822.270696	340261.174766	37.563776
1824.281572	340927.718042	37.568794
1826.049618	341606.984132	37.573812
1827.860277	342288.315422	37.578829
1829.468092	342975.331142	37.583847
1831.297251	343650.371326	37.588864
1833.274905	344345.936836	37.593882
1835.173819	345027.545747	37.598900
1837.234973	345707.493919	37.603917
1839.513856	346393.157918	37.608935
1841.048089	347069.721884	37.613952
1843.000708	347745.572654	37.618970
1844.973404	348450.266743	37.623988
1846.423810	349139.149044	37.629005
1848.568473	349808.745669	37.634023
1850.515049	350521.203675	37.639040
1852.448367	351191.271666	37.644058
1853.842471	351891.820866	37.649076
1855.834657	352574.877143	37.654093
1857.879784	353265.552562	37.659111
1859.637608	353965.171622	37.664128
1862.053733	354647.643686	37.669146
1863.747685	355331.492914	37.674164
1866.069107	356007.412265	37.679181
1868.167383	356691.680641	37.684199
1869.495902	357374.491759	37.689216
1871.384587	358058.493495	37.694234
1873.476140	358726.338458	37.699252
1875.353990	359393.040786	37.704269
1877.393027	360039.889735	37.709287
1879.036245	360701.966377	37.714304
1880.877587	361353.343421	37.719322
1882.657024	362009.388541	37.724340
1884.281275	362652.864544	37.729357
1886.383607	363327.381051	37.734375
1887.806736	363987.892326	37.739392
1889.997778	364659.428568	37.744410
1891.926184	365327.064385	37.749428
1893.503450	365996.243441	37.754445
1895.430976	366670.299997	37.759463
1897.119107	367361.710542	37.764480
1899.330329	368034.148875	37.769498
1900.892414	368721.395258	37.774516
1902.837646	369409.073256	37.779533
1904.463313	370103.361171	37.784551
1906.374019	370796.143289	37.789568
1908.256285	371505.024004	37.794586
1909.682423	372201.258589	37.799604
1911.576310	372918.683305	37.804621
1913.838475	373639.913741	37.809639
1915.006651	374361.716006	37.814656
1916.909015	375084.828313	37.819674
1919.156798	375827.676779	37.824692
1920.807392	376556.380297	37.829709
1922.785300	377292.623043	37.834727
1924.473135	378044.165145	37.839744
1926.187794	378788.357522	37.844762
1927.820885	379548.498364	37.849780
1929.664775	380312.087094	37.854797
1931.927817	381066.562021	37.859815
1933.676646	381839.793555	37.864832
1935.887212	382605.273298	37.869850
1937.719236	383371.533268	37.874868
1940.039207	384154.607476	37.879885
1942.183575	384908.026305	37.884903
1943.916141	385680.461091	37.889920
1945.978049	386468.263909	37.894938
1947.846705	387238.433373	37.899956
1949.833882	388008.539494	37.904973
1951.918982	388811.492839	37.909991
1953.754449	389591.726631	37.915008
1956.002942	390370.453362	37.920026
1957.953260	391151.237977	37.925044
1959.768996	391943.103088	37.930061
1962.136170	392718.430800	37.935079
1963.583421	393519.594072	37.940096
1965.401556	394309.978451	37.945114
1967.567686	395105.227610	37.950132
1969.548476	395902.792968	37.955149
1971.572411	396700.760943	37.960167
1973.232981	397490.581082	37.965184
1975.297149	398287.359431	37.970202
1977.727476	399086.640973	37.975220
1979.292125	399902.263100	37.980237
1981.492960	400700.220627	37.985255
1983.221238	401512.754931	37.990272
1985.325860	402322.391458	37.995290
1987.524592	403116.354709	38.000308
1989.353060	403931.464754	38.005325
1991.537644	404736.154435	38.010343
1993.821072	405539.892694	38.015360
1995.705437	406339.670446	38.020378
1998.422008	407138.806628	38.025396
2000.411501	407932.769841	38.030413
2002.755616	408716.441659	38.035431
2004.739962	409498.123681	38.040448
2006.790745	410258.340040	38.045466
2009.161132	411009.413188	38.050484
2011.011895	411762.907064	38.055501
2012.936044	412503.625921	38.060519
2015.135141	413253.043421	38.065536
2016.845277	414012.576550	38.070554
2019.005438	414770.291279	38.075572
2020.807587	415535.641886	38.080589
2022.667675	416282.471169	38.085607
2024.744474	417055.988927	38.090624
2026.543294	417817.068849	38.095642
2028.540727	418592.605254	38.100660
2030.268894	419370.112695	38.105677
2032.295023	420132.960623	38.110695
2034.271083	420911.139959	38.115712
2036.231022	421694.084031	38.120730
2038.472815	422490.276602	38.125748
2040.306001	423290.081552	38.130765
2042.587346	424056.592113	38.135783
2044.935019	424848.286271	38.140800
2046.815038	425648.615209	38.145818
2049.458582	426438.158704	38.150836
2050.951546	427243.056670	38.155853
2052.979228	428041.966509	38.160871
2054.542155	428853.229901	38.165888
2056.611626	429666.559516	38.170906
2058.699515	430479.504140	38.175924
2060.353841	431307.123346	38.180941
2062.803941	432114.940512	38.185959
2064.743158	432952.377546	38.190976
2066.712683	433778.440880	38.195994
2069.070599	434600.564033	38.201012
2071.087510	435442.201787	38.206029
2073.293620	436275.173304	38.211047
2075.354088	437118.716862	38.216064
2077.179891	437959.433927	38.221082
2079.333837	438799.458649	38.226100
2080.850463	439665.518955	38.231117
2082.930163	440519.156198	38.236135
2085.322257	441372.962593	38.241152
2087.057592	442234.232581	38.246170
2089.233602	443104.049157	38.251188
2090.984005	443975.875143	38.256205
2093.366455	444856.416701	38.261223
2095.254753	445729.516660	38.266240
2097.475563	446604.095282	38.271258
2099.633056	447475.107964	38.276276
2101.688798	448361.430371	38.281293
2104.032768	449231.178045	38.286311
2106.361315	450129.775996	38.291328
2108.152203	451005.157549	38.296346
2110.529500	451896.288146	38.301364
2112.027807	452796.832289	38.306381
2114.384122	453676.713725	38.311399
2116.985697	454565.974837	38.316416
2118.919434	455477.103969	38.321434
2121.357764	456355.695770	38.326452
2123.521031	457253.460073	38.331469
2125.808737	458134.175263	38.336487
2127.900892	459019.536485	38.341504
2129.671533	459911.484990	38.346522
2131.779070	460807.433864	38.351540
2133.953597	461707.022456	38.356557
2136.121501	462592.214949	38.361575
2138.000553	463495.512958	38.366592
2140.445250	464394.632899	38.371610
2142.715839	465283.833817	38.376628
2145.035819	466178.697962	38.381645
2146.699403	467040.626189	38.386663
2149.350620	467908.266672	38.391680
2150.950344	468786.856780	38.396698
2153.483500	469656.308595	38.401716
2154.781635	470514.403592	38.406733
2157.036129	471384.834059	38.411751
2159.319742	472284.374604	38.416768
2161.054183	473159.408039	38.421786
2163.289685	474032.600768	38.426804
2165.462414	474937.338874	38.431821
2167.802368	475824.930833	38.436839
2169.573901	476708.078614	38.441856
2171.843974	477630.199708	38.446874
2174.021417	478522.539511	38.451892
2176.180898	479441.911731	38.456909
2178.236453	480349.335880	38.461927
2180.090163	481271.798435	38.466944
2182.034816	482195.916471	38.471962
2184.878415	483109.689232	38.476980
2187.930802	484050.952063	38.481997
2189.994138	484965.820086	38.487015
2192.601156	485885.348470	38.492032
2194.584748	486812.404582	38.497050
2196.841804	487739.367373	38.502068
2198.916009	488675.449215	38.507085
2201.217775	489589.384266	38.512103
2203.424158	490509.698178	38.517120
2205.543612	491451.480230	38.522138
2207.738313	492366.650886	38.527156
2209.732655	493317.689923	38.532173
2212.417564	494260.891955	38.537191
2214.613980	495187.570856	38.542208
2216.417985	496129.554060	38.547226
2218.773026	497074.169687	38.552244
2221.130082	498039.015540	38.557261
2223.222733	498985.586336	38.562279
2225.885025	499928.730911	38.567296
2227.950688	500897.800066	38.572314
2230.151283	501835.818445	38.577332
2232.319778	502794.066585	38.582349
2234.584617	503750.780846	38.587367
2236.847615	504719.897513	38.592384
2239.050749	505681.099634	38.597402
2241.319222	506654.186347	38.602420
2242.924644	507626.568036	38.607437
2245.059115	508593.862936	38.612455
2247.793727	509571.185983	38.617472
2249.742676	510547.419792	38.622490
2251.900262	511548.968478	38.627508
2254.309023	512520.620382	38.632525
2255.819522	513526.134255	38.637543
2258.117562	514520.214441	38.642560
2260.324179	515513.087980	38.647578
2263.337868	516510.956849	38.652596
2265.238248	517519.931844	38.657613
2267.385668	518526.331762	38.662631
2269.732841	519535.959270	38.667648
2271.674739	520561.811753	38.672666
2273.816334	521563.631877	38.677684
2276.499569	522594.718307	38.682701
2278.390497	523612.214328	38.687719
2281.085778	524633.136574	38.692736
2283.035359	525650.889560	38.697754
2285.437434	526672.327173	38.702772
2287.444295	527702.775346	38.707789
2289.244234	528738.021212	38.712807
2292.031005	529760.041249	38.717824
2294.083920	530796.311023	38.722842
2296.343681	531807.149551	38.727860
2298.646509	532814.790456	38.732877
2300.925778	533820.000212	38.737895
2303.183986	534829.674810	38.742912
2304.963575	535844.039491	38.747930
2307.317986	536854.715544	38.752948
2309.975952	537877.500352	38.757965
2312.331948	538886.574613	38.762983
2315.232944	539900.469792	38.768000
2317.287240	540939.339056	38.773018
2319.320278	541965.155658	38.778036
2321.616808	542987.081633	38.783053
2323.524703	544035.256995	38.788071
2326.067916	545082.243685	38.793088
2327.678027	546125.885961	38.798106
2330.283025	547181.708868	38.803124
2332.835352	548228.710080	38.808141
2334.758887	549298.817195	38.813159
2337.246194	550363.217574	38.818176
2339.657765	551436.899913	38.823194
2341.626105	552509.565853	38.828212
2344.331140	553587.354813	38.833229
2346.450333	554677.017846	38.838247
2349.024738	555770.438746	38.843264
2350.815651	556876.464811	38.848282
2353.564642	557968.120752	38.853300
2355.733661	559073.551828	38.858317
2358.064533	560193.033945	38.863335
2360.329462	561291.230944	38.868352
2362.717757	562428.451229	38.873370
2365.172278	563542.154213	38.878388
2367.412255	564667.853051	38.883405
2369.304992	565796.576059	38.888423
2371.850079	566937.146601	38.893440
2374.279887	568090.541347	38.898458
2376.965088	569226.418300	38.903476
2379.142211	570370.311954	38.908493
2381.164701	571533.356512	38.913511
2384.214122	572680.364119	38.918528
2386.101013	573839.456175	38.923546
2388.129498	574996.210783	38.928564
2391.353456	576176.700354	38.933581
2393.592632	577339.729229	38.938599
2396.367497	578502.712493	38.943616
2398.386628	579680.411732	38.948634
2400.750780	580852.374404	38.953652
2403.072175	582033.161807	38.958669
2405.358280	583214.694780	38.963687
2407.887745	584392.964853	38.968704
2410.090689	585587.924018	38.973722
2412.410329	586772.969600	38.978740
2414.677598	587958.560096	38.983757
2417.060031	589169.933086	38.988775
2419.447773	590363.138400	38.993792
2421.929540	591572.699424	38.998810
2423.907628	592777.861243	39.003828
2426.607081	593989.497168	39.008845
2428.903686	595224.074211	39.013863
2431.541367	596422.895249	39.018880
2434.132663	597637.983057	39.023898
2436.510422	598861.295225	39.028916
2439.075139	600080.542066	39.033933
2441.600005	601302.422263	39.038951
2443.895590	602519.104110	39.043968
2446.125004	603742.478198	39.048986
2448.773200	604964.702144	39.054004
2451.222367	606191.934642	39.059021
2453.105796	607420.179776	39.064039
2456.213102	608609.204038	39.069056
2458.726381	609797.551072	39.074074
2461.623969	610972.400060	39.079092
2464.433736	612165.702706	39.084109
2466.591438	613327.269313	39.089127
2469.062484	614501.369010	39.094144
2471.535070	615685.047831	39.099162
2473.813105	616874.183716	39.104180
2476.421735	618061.737181	39.109197
2478.191960	619259.000870	39.114215
2480.627630	620468.622930	39.119232
2483.357557	621678.112809	39.124250
2485.604318	622878.551266	39.129268
2488.351033	624092.118712	39.134285
2490.532315	625307.492317	39.139303
2493.531807	626531.238311	39.144320
2495.872190	627758.201077	39.149338
2498.619962	628968.271277	39.154356
2500.847850	630198.269624	39.159373
2503.413889	631434.612562	39.164391
2506.225357	632648.448780	39.169408
2509.061697	633883.212537	39.174426
2511.384096	635117.017446	39.179444
2514.118317	636357.747836	39.184461
2516.256874	637593.587411	39.189479
2519.065718	638831.166123	39.194496
2521.388194	640078.957168	39.199514
2524.084197	641340.357191	39.204532
2526.790731	642584.438891	39.209549
2529.214643	643845.426723	39.214567
2531.614086	645098.182936	39.219584
2534.549007	646354.586849	39.224602
2537.778324	647588.796156	39.229620
2540.719122	648840.901632	39.234637
2542.674912	650094.110740	39.239655
2545.424350	651345.188412	39.244672
2547.613904	652604.575248	39.249690
2549.679216	653868.109355	39.254708
2552.377541	655137.557213	39.259725
2554.710262	656409.493392	39.264743
2557.233645	657693.538573	39.269760
2559.665914	658981.316237	39.274778
2562.050566	660265.446463	39.279796
2564.590802	661554.859728	39.284813
2566.562090	662870.086037	39.289831
2568.973993	664164.401960	39.294848
2571.538123	665488.882283	39.299866
2573.912262	666799.724592	39.304884
2576.278769	668124.969203	39.309901
2578.554342	669477.161283	39.314919
2581.100386	670806.531620	39.319936
2584.048936	672157.584947	39.324954
2586.505328	673505.741360	39.329972
2589.356498	674860.551793	39.334989
2592.001330	676206.848015	39.340007
2594.552531	677548.342792	39.345024
2597.403732	678899.038990	39.350042
2599.957471	680266.882491	39.355060
2602.490583	681601.036295	39.360077
2605.122984	682964.542022	39.365095
2607.910918	684324.740001	39.370112
2610.570370	685678.598346	39.375130
2613.376905	687035.310586	39.380148
2616.435881	688372.960282	39.385165
2618.844825	689731.519870	39.390183
2621.881046	691071.753009	39.395200
2624.559395	692435.767655	39.400218
2626.446192	693758.319395	39.405236
2629.661997	695079.166413	39.410253
2631.977852	696398.031144	39.415271
2634.536850	697705.449960	39.420288
2637.542038	699011.907741	39.425306
2639.686197	700323.024628	39.430324
2641.926779	701630.062882	39.435341
2644.248366	702965.148803	39.440359
2647.020082	704293.661740	39.445376
2649.221341	705638.617801	39.450394
2651.295401	706982.989881	39.455412
2654.141739	708342.779698	39.460429
2656.399767	709707.900477	39.465447
2658.801387	711071.641448	39.470464
2661.613211	712459.360977	39.475482
2663.913072	713851.394845	39.480500
2666.485976	715230.730881	39.485517
2669.154086	716642.442449	39.490535
2671.871645	718045.695239	39.495552
2674.841244	719469.254487	39.500570
2677.531496	720885.049337	39.505588
2680.049847	722295.933827	39.510605
2682.576507	723737.484674	39.515623
2685.123191	725172.156363	39.520640
2688.204954	726611.631916	39.525658
2690.654346	728056.792210	39.530676
2693.605682	729501.812956	39.535693
2696.241671	730961.749036	39.540711
2699.064214	732408.203356	39.545728
2701.809083	733877.675449	39.550746
2704.140451	735340.825610	39.555764
2707.377622	736802.227974	39.560781
2710.028098	738275.950016	39.565799
2712.701969	739747.274757	39.570816
2716.071144	741216.634574	39.575834
2718.580066	742698.050460	39.580852
2721.351642	744155.568144	39.585869
2723.885833	745644.665454	39.590887
2726.483940	747131.646052	39.595904
2729.329644	748611.402092	39.600922
2731.772012	750113.469415	39.605940
2734.687326	751606.791556	39.610957
2737.390208	753106.364920	39.615975
2740.175203	754594.451830	39.620992
2742.915378	756101.368044	39.626010
2745.982431	757615.567012	39.631028
2749.009418	759117.706637	39.636045
2751.674263	760622.858627	39.641063
2754.357852	762124.067713	39.646080
2757.103864	763629.347884	39.651098
2759.835026	765140.676031	39.656116
2762.537212	766653.475781	39.661133
2765.111645	768165.597828	39.666151
2767.607963	769696.157431	39.671168
2770.222151	771230.560787	39.676186
2772.773674	772762.101643	39.681204
2775.620350	774295.340029	39.686221
2778.328640	775850.337534	39.691239
2780.986135	777390.820889	39.696256
2783.708716	778939.316161	39.701274
2786.238926	780498.461234	39.706292
2788.633663	782064.852186	39.711309
2791.483747	783638.238503	39.716327
2794.094037	785205.777521	39.721344
2796.953619	786766.459315	39.726362
2799.997941	788342.756516	39.731380
2803.147004	789923.051580	39.736397
2805.685154	791504.027428	39.741415
2808.149026	793074.862075	39.746432
2811.443531	794617.382389	39.751450
2813.922722	796164.891111	39.756468
2816.733235	797700.838317	39.761485
2819.415768	799236.224347	39.766503
2821.884717	800773.558936	39.771520
2824.964199	802329.489925	39.776538
2827.491911	803882.275242	39.781556
2830.645550	805431.672818	39.786573
2833.024119	806996.547679	39.791591
2835.492388	808569.362431	39.796608
2838.348870	810140.822119	39.801626
2841.092967	811720.392257	39.806644
2843.870547	813311.559790	39.811661
2846.833488	814915.706760	39.816679
2849.561392	816514.138242	39.821696
2852.531848	818117.861679	39.826714
2854.699360	819734.756706	39.831732
2857.352006	821361.916046	39.836749
2860.416884	822997.244682	39.841767
2863.471874	824655.486660	39.846784
2866.674886	826303.241674	39.851802
2869.167108	827946.459184	39.856820
2872.133865	829593.183052	39.861837
2875.093947	831257.132310	39.866855
2877.713285	832933.767921	39.871872
2880.951694	834595.159418	39.876890
2883.391140	836270.618973	39.881908
2886.126092	837949.536643	39.886925
2889.267017	839639.578923	39.891943
2892.124502	841328.247924	39.896960
2895.264913	843014.136490	39.901978
2897.897950	844713.227543	39.906996
2900.841214	846417.255669	39.912013
2903.839168	848131.019987	39.917031
2906.543920	849843.684657	39.922048
2909.325225	851556.353667	39.927066
2912.312846	853281.435186	39.932084
2914.987552	855011.040988	39.937101
2917.987976	856731.276925	39.942119
2920.654097	858480.296794	39.947136
2923.904024	860218.051644	39.952154
2926.723959	861978.078290	39.957172
2929.751104	863714.584897	39.962189
2932.702007	865475.712346	39.967207
2935.555714	867236.634652	39.972224
2938.711828	868987.500249	39.977242
2941.363423	870764.571035	39.982260
2944.297618	872517.058760	39.987277
2947.346865	874294.661413	39.992295
2950.230007	876055.505540	39.997312
2953.380934	877827.583499	40.002330
2956.558331	879612.373345	40.007348
2959.352990	881388.661793	40.012365
2962.201361	883164.983524	40.017383
2964.867933	884943.404029	40.022400
2968.298573	886732.648862	40.027418
2971.377392	888517.248491	40.032436
2974.014741	890305.520678	40.037453
2977.115080	892084.767131	40.042471
2979.760935	893880.224987	40.047488
2983.018190	895670.775959	40.052506
2985.306052	897477.794423	40.057524
2988.513391	899269.438752	40.062541
2991.527363	901083.283928	40.067559
2994.409281	902886.262876	40.072576
2997.875311	904677.976985	40.077594
3000.671599	906498.102089	40.082612
3003.730855	908295.268774	40.087629
3006.638013	910057.927122	40.092647
3009.253259	911833.630703	40.097664
3012.117621	913603.147438	40.102682
3014.844903	915373.271110	40.107700
3017.664864	917149.148392	40.112717
3020.176539	918933.238271	40.117735
3023.039528	920737.517467	40.122752
3025.905346	922526.897849	40.127770
3028.797323	924342.159685	40.132788
3031.785533	926158.137126	40.137805
3034.949715	927979.607330	40.142823
3037.313031	929821.290148	40.147840
3040.617311	931653.943284	40.152858
3043.548319	933501.157557	40.157876
3046.691012	935358.989552	40.162893
3049.926670	937216.343721	40.167911
3052.278097	939085.720054	40.172928
3055.726643	940949.754166	40.177946
3058.505222	942846.692725	40.182964
3061.491977	944732.584614	40.187981
3064.503219	946629.345438	40.192999
3067.478423	948536.588477	40.198016
3070.573882	950445.300524	40.203034
3073.626472	952370.294353	40.208052
3076.270662	954300.448802	40.213069
3079.526725	956272.474965	40.218087
3082.434901	958258.853681	40.223104
3085.939729	960247.090297	40.228122
3089.374265	962248.922558	40.233140
3092.084503	964245.000239	40.238157
3095.067328	966241.219851	40.243175
3098.790195	968261.033439	40.248192
3101.401236	970280.222431	40.253210
3104.786508	972298.573617	40.258228
3107.611386	974314.648664	40.263245
3110.747168	976333.083018	40.268263
3114.178254	978369.080058	40.273280
3117.802422	980408.607227	40.278298
3120.460969	982443.864385	40.283316
3123.567521	984478.224722	40.288333
3126.994713	986525.334530	40.293351
3129.797747	988570.935956	40.298368
3132.736106	990620.642645	40.303386
3135.802618	992665.797872	40.308404
3138.591466	994726.783841	40.313421
3142.565441	996777.111362	40.318439
3145.897226	998830.396378	40.323456
3149.460370	1000877.462637	40.328474
3152.902423	1002941.470167	40.333492
3156.078012	1004990.313968	40.338509
3159.445677	1007028.976635	40.343527
3162.515545	1009077.130284	40.348544
3165.917844	1011130.396142	40.353562
3169.047769	1013180.342935	40.358580
3172.221824	1015216.657058	40.363597
3175.609469	1017248.326523	40.368615
3178.497438	1019301.888764	40.373632
3181.416797	1021354.597561	40.378650
3184.585426	1023406.900408	40.383668
3187.754652	1025458.451054	40.388685
3190.719794	1027512.568108	40.393703
3193.748127	1029582.145986	40.398720
3197.054269	1031642.318312	40.403738
3199.915705	1033718.499693	40.408756
3202.456128	1035792.609891	40.413773
3205.602171	1037878.867182	40.418791
3208.276721	1039972.806790	40.423808
3211.193706	1042054.931594	40.428826
3214.193760	1044116.224840	40.433844
3216.989488	1046182.659689	40.438861
3220.581647	1048255.989739	40.443879
3223.488749	1050327.597506	40.448896
3226.370047	1052396.413526	40.453914
3229.127751	1054475.724931	40.458932
3232.181724	1056571.504916	40.463949
3235.436963	1058681.443341	40.468967
3238.195740	1060801.892119	40.473984
3241.327702	1062911.573888	40.479002
3244.289034	1065058.381142	40.484020
3246.962925	1067216.291728	40.489037
3250.264127	1069370.085784	40.494055
3253.428734	1071549.511430	40.499072
3256.444649	1073728.573007	40.504090
3259.845201	1075920.015983	40.509108
3262.517845	1078126.783783	40.514125
3266.005543	1080347.167040	40.519143
3268.792947	1082578.144812	40.524160
3272.335226	1084805.789442	40.529178
3275.278760	1087061.868329	40.534196
3278.163450	1089324.472524	40.539213
3281.825257	1091598.038833	40.544231
3284.756118	1093875.736168	40.549248
3287.607808	1096157.832349	40.554266
3290.996113	1098458.144473	40.559284
3294.368975	1100762.151691	40.564301
3297.779313	1103054.210028	40.569319
3300.712929	1105382.618610	40.574336
3304.429496	1107695.418834	40.579354
3307.869129	1110023.164832	40.584372
3311.018548	1112352.043394	40.589389
3314.855186	1114677.135879	40.594407
3318.055819	1117029.175062	40.599424
3321.498565	1119363.039773	40.604442
3324.649324	1121710.464656	40.609460
3328.250879	1124046.627032	40.614477
3331.804650	1126395.722942	40.619495
3335.305661	1128752.897505	40.624512
3338.667600	1131092.745867	40.629530
3342.051766	1133445.396285	40.634548
3345.294767	1135798.543769	40.639565
3348.737467	1138153.834044	40.644583
3351.924814	1140517.961815	40.649600
3355.174890	1142875.253744	40.654618
3358.777219	1145242.593811	40.659636
3361.639578	1147609.845462	40.664653
3365.166944	1149982.538153	40.669671
3368.302749	1152355.171426	40.674688
3371.266004	1154743.185713	40.679706
3374.518323	1157125.822884	40.684724
3377.536285	1159536.931351	40.689741
3381.001561	1161935.453921	40.694759
3384.392859	1164341.557679	40.699776
3387.535597	1166753.281718	40.704794
3391.237370	1169173.683511	40.709812
3394.636072	1171589.344198	40.714829
3397.642127	1174008.087942	40.719847
3400.953542	1176440.884253	40.724864
3404.276117	1178863.146717	40.729882
3407.840735	1181305.085881	40.734900
3411.073010	1183752.969905	40.739917
3414.484146	1186178.279562	40.744935
3418.004624	1188633.190640	40.749952
3421.193193	1191073.776024	40.754970
3424.792623	1193522.320899	40.759988
3428.135271	1195969.277580	40.765005
3431.270157	1198384.379050	40.770010
3434.686802	1200771.491941	40.775015
3437.642504	1203085.858954	40.780020
3440.881680	1205352.941143	40.785024
3443.902644	1207532.420349	40.790029
3446.901652	1209646.844231	40.795034
3450.552908	1211678.680489	40.800039
3453.279341	1213626.695625	40.805044
3456.503966	1215494.584459	40.810048
3458.977485	1217287.220378	40.815053
3461.737515	1218993.951124	40.820058
3464.127944	1220635.896850	40.825063
3466.517191	1222198.583101	40.830068
3469.232942	1223678.573888	40.835072
3471.772845	1225096.931833	40.840077
3473.618649	1226428.411850	40.845082
3475.734487	1227704.176142	40.850087
3477.607002	1228907.935538	40.855092
3479.694453	1230037.707428	40.860096
3481.391366	1231133.636054	40.865101
3483.164831	1232151.578240	40.870106
3484.983761	1233113.765799	40.875111
3486.363894	1234009.501812	40.880116
3487.845652	1234859.600418	40.885120
3489.442422	1235667.342433	40.890125
3491.243380	1236401.348188	40.895130
3492.146668	1237106.062723	40.900135
3493.512602	1237763.956547	40.905140
3494.723069	1238372.077562	40.910144
3495.939342	1238950.151140	40.915149
3497.202925	1239480.775823	40.920154
3498.115019	1239989.625262	40.925159
3499.006516	1240441.010890	40.930164
3500.467599	1240863.882352	40.935168
3501.264229	1241254.170100	40.940173
3502.160802	1241596.777143	40.945178
3502.704874	1241923.696942	40.950183
3503.473069	1242216.697934	40.955188
3504.499300	1242475.780453	40.960192
3504.975319	1242723.871487	40.965197
3505.896780	1242947.973267	40.970202
3506.434139	1243126.368943	40.975207
3506.785751	1243293.628388	40.980212
3507.710959	1243444.326590	40.985216
3508.358448	1243572.374296	40.990221
3508.811070	1243668.738874	40.995226
3509.302815	1243745.101100	41.000231
3509.563154	1243816.013600	41.005236
3510.340397	1243868.892259	41.010240
3510.849839	1243896.520426	41.015245
3511.351850	1243900.064550	41.020250
3511.784843	1243916.546031	41.025255
3512.122897	1243903.750424	41.030260
3512.944245	1243853.491829	41.035264
3512.918332	1243806.999054	41.040269
3513.458091	1243751.392121	41.045274
3513.881821	1243688.642932	41.050279
3513.836969	1243584.771844	41.055284
3514.486635	1243488.317288	41.060288
3514.297477	1243400.834236	41.065293
3514.627684	1243254.950425	41.070298
3515.045472	1243142.623578	41.075303
3515.205439	1243009.223595	41.080308
3515.727221	1242858.460255	41.085312
3515.560397	1242713.572726	41.090317
3515.802712	1242536.894564	41.095322
3516.217694	1242377.111633	41.100327
3516.139489	1242198.427911	41.105332
3516.355934	1242015.782156	41.110336
3516.692384	1241837.203382	41.115341
3517.125209	1241646.787028	41.120346
3517.193653	1241434.745560	41.125351
3517.030548	1241221.058530	41.130356
3517.318152	1241010.451782	41.135360
3517.398701	1240795.124764	41.140365
3517.453901	1240564.531788	41.145370
3517.458527	1240343.800811	41.150375
3517.934899	1240112.931690	41.155380
3518.120429	1239867.488323	41.160384
3517.661965	1239622.511344	41.165389
3518.279398	1239373.622208	41.170394
3518.325874	1239121.556975	41.175399
3518.781246	1238863.268127	41.180404
3518.777747	1238581.210330	41.185408
3518.957756	1238319.587701	41.190413
3518.945214	1238051.559246	41.195418
3519.372250	1237778.602647	41.200423
3519.029911	1237497.098649	41.205428
3519.313784	1237217.524371	41.210432
3519.107903	1236924.978229	41.215437
3519.345360	1236637.184724	41.220442
3519.486515	1236350.321994	41.225447
3519.367772	1236063.858314	41.230452
3519.522520	1235761.964730	41.235456
3519.287507	1235471.667720	41.240461
3519.305625	1235169.295459	41.245466
3519.720531	1234866.932913	41.250471
3519.645591	1234561.558488	41.255476
3519.578022	1234262.034158	41.260480
3519.259127	1233958.433696	41.265485
3519.630823	1233646.594415	41.270490
3519.435628	1233350.298439	41.275495
3519.324528	1233048.659230	41.280500
3519.782508	1232733.394461	41.285504
3519.647505	1232426.409721	41.290509
3519.883214	1232107.227932	41.295514
3519.549381	1231804.339442	41.300519
3519.721600	1231482.518643	41.305524
3519.799619	1231161.718401	41.310528
3519.504580	1230856.342835	41.315533
3519.846976	1230536.205280	41.320538
3520.105516	1230221.376284	41.325543
3519.960204	1229890.741505	41.330548
3520.071557	1229569.834898	41.335552
3519.801892	1229247.944811	41.340557
3520.010143	1228909.167079	41.345562
3519.725669	1228591.061737	41.350567
3519.637727	1228273.650305	41.355572
3520.065565	1227938.596060	41.360576
3519.668609	1227614.850716	41.365581
3519.681629	1227282.247035	41.370586
3519.756895	1226962.020913	41.375591
3519.620579	1226627.252844	41.380596
3519.691765	1226304.373152	41.385600
3519.728629	1225991.277509	41.390605
3519.768588	1225649.603299	41.395610
3519.639872	1225324.267595	41.400615
3519.563501	1224992.275170	41.405620
3519.814503	1224659.740381	41.410624
3519.223538	1224349.167214	41.415629
3519.514426	1224005.287231	41.420634
3519.598781	1223686.346652	41.425639
3519.558568	1223366.659592	41.430644
3519.524521	1223025.194441	41.435648
3519.500744	1222694.350417	41.440653
3519.535889	1222358.992437	41.445658
3519.790337	1222025.817726	41.450663
3519.411436	1221684.879697	41.455668
3519.853347	1221343.223177	41.460672
3519.405332	1221018.318093	41.465677
3519.554578	1220687.128129	41.470682
3519.956330	1220358.864682	41.475687
3519.373839	1220025.323053	41.480692
3519.395397	1219684.371836	41.485696
3519.426482	1219358.440888	41.490701
3519.583942	1219016.114306	41.495706
3519.346948	1218675.511910	41.500711
3518.989189	1218343.131429	41.505716
3519.212026	1218012.035685	41.510720
3519.099689	1217688.732112	41.515725
3519.103703	1217358.658182	41.520730
3519.385924	1217034.126324	41.525735
3519.411568	1216707.933176	41.530740
3519.531159	1216363.751721	41.535744
3518.907533	1216039.866749	41.540749
3519.203450	1215692.618767	41.545754
3519.073901	1215366.271835	41.550759
3518.795751	1215046.475190	41.555764
3519.390669	1214710.895183	41.560768
3519.099404	1214373.661866	41.565773
3518.913384	1214034.705162	41.570778
3518.966278	1213715.331831	41.575783
3518.910201	1213379.116653	41.580788
3518.920975	1213047.639930	41.585792
3518.785004	1212712.703886	41.590797
3518.993791	1212388.169272	41.595802
3518.878674	1212059.924235	41.600807
3518.808282	1211736.891496	41.605812
3519.031684	1211397.411559	41.610816
3518.616110	1211074.768180	41.615821
3518.703856	1210738.261913	41.620826
3518.616992	1210400.264511	41.625831
3518.787950	1210077.742446	41.630836
3518.878604	1209747.629964	41.635840
3518.606658	1209419.428441	41.640845
3518.375765	1209094.476260	41.645850
3518.456623	1208758.589956	41.650855
3518.096240	1208442.326133	41.655860
3518.830745	1208118.744986	41.660864
3518.233040	1207793.583315	41.665869
3518.254790	1207467.081354	41.670874
3518.014752	1207145.191464	41.675879
3518.314367	1206823.098796	41.680884
3518.494292	1206505.970665	41.685888
3518.108026	1206187.042426	41.690893
3518.129052	1205853.786036	41.695898
3518.701242	1205540.187555	41.700903
3518.430409	1205210.310535	41.705908
3518.362653	1204867.259401	41.710912
3517.876685	1204555.086888	41.715917
3518.126197	1204216.625790	41.720922
3517.926925	1203902.023254	41.725927
3518.004919	1203588.480570	41.730932
3518.190600	1203266.558173	41.735936
3517.999430	1202947.208779	41.740941
3517.733274	1202620.726758	41.745946
3517.694872	1202302.905896	41.750951
3517.617623	1201991.260118	41.755956
3517.853797	1201666.134881	41.760960
3517.886140	1201342.241710	41.765965
3517.783299	1201025.196369	41.770970
3517.992436	1200722.710739	41.775975
3517.706636	1200391.963671	41.780980
3518.054793	1200067.656781	41.785984
3517.273169	1199743.703102	41.790989
3517.467268	1199426.697857	41.795994
3517.427749	1199115.809553	41.800999
3517.602377	1198796.892393	41.806004
3517.822245	1198481.419613	41.811008
3517.722609	1198164.103456	41.816013
3517.222198	1197843.080187	41.821018
3517.488175	1197539.553405	41.826023
3517.390407	1197219.081811	41.831028
3517.848709	1196902.628346	41.836032
3517.280377	1196592.894813	41.841037
3517.318852	1196271.497049	41.846042
3517.732059	1195951.050123	41.851047
3517.372183	1195637.000472	41.856052
3517.263667	1195326.927310	41.861056
3517.068835	1195014.126889	41.866061
3517.206868	1194688.482808	41.871066
3517.269401	1194387.245064	41.876071
3517.140668	1194075.409707	41.881076
3517.283310	1193759.472539	41.886080
3517.052916	1193452.781485	41.891085
3517.401516	1193136.960109	41.896090
3517.090346	1192826.676002	41.901095
3517.035821	1192515.955221	41.906100
3516.883821	1192209.271258	41.911104
3516.597663	1191905.597460	41.916109
3516.870834	1191585.278047	41.921114
3516.554837	1191280.350994	41.926119
3516.650276	1190987.177584	41.931124
3516.705373	1190682.811875	41.936128
3516.707821	1190375.429716	41.941133
3516.649778	1190075.933560	41.946138
3516.966999	1189771.658964	41.951143
3516.402356	1189464.221996	41.956148
3516.991261	1189157.986711	41.961152
3516.946568	1188856.913760	41.966157
3516.514474	1188536.145418	41.971162
3516.733467	1188226.907655	41.976167
3516.252249	1187939.015037	41.981172
3516.567191	1187622.485875	41.986176
3516.540405	1187326.680280	41.991181
3516.611587	1187016.924377	41.996186
3516.435800	1186710.952255	42.001191
3516.417609	1186411.613406	42.006196
3516.480445	1186115.159517	42.011200
3516.102373	1185817.914746	42.016205
3516.105586	1185514.287897	42.021210
3515.892117	1185217.639993	42.026215
3515.904067	1184918.774274	42.031220
3516.110520	1184624.281003	42.036224
3516.156260	1184344.568706	42.041229
3515.871055	1184043.725676	42.046234
3515.849610	1183743.104024	42.051239
3515.899961	1183445.934833	42.056244
3516.134387	1183145.706903	42.061248
3515.729553	1182863.824453	42.066253
3516.013290	1182567.413475	42.071258
3516.057538	1182265.095320	42.076263
3515.794438	1181972.975916	42.081268
3515.743350	1181681.275805	42.086272
3515.340068	1181389.523156	42.091277
3515.566994	1181093.131439	42.096282
3515.611569	1180812.569770	42.101287
3515.135737	1180530.289725	42.106292
3515.413018	1180240.714242	42.111296
3515.617922	1179958.385151	42.116301
3515.711285	1179665.417984	42.121306
3515.543348	1179379.634576	42.126311
3515.542796	1179102.660740	42.131316
3515.481683	1178807.504501	42.136320
3515.602297	1178515.786596	42.141325
3515.649314	1178221.709556	42.146330
3515.396593	1177945.940127	42.151335
3514.964801	1177652.569136	42.156340
3515.485898	1177364.300465	42.161344
3515.717514	1177091.232255	42.166349
3515.314561	1176799.975363	42.171354
3515.448627	1176510.780920	42.176359
3514.991010	1176228.075582	42.181364
3515.251653	1175940.147812	42.186368
3514.969873	1175661.623376	42.191373
3515.336176	1175369.028767	42.196378
3515.401388	1175092.867169	42.201383
3514.909661	1174811.787019	42.206388
3515.213786	1174526.036034	42.211392
3514.675213	1174244.932987	42.216397
3514.979150	1173974.517323	42.221402
3515.150329	1173693.550441	42.226407
3514.842071	1173408.687502	42.231412
3514.853045	1173122.436382	42.236416
3514.508558	1172869.890501	42.241421
3514.883797	1172591.565062	42.246426
3515.124822	1172315.038612	42.251431
3514.956570	1172034.981223	42.256436
3514.769043	1171750.102027	42.261440
3514.830168	1171471.957178	42.266445
3514.678720	1171183.457015	42.271450
3515.096041	1170915.316341	42.276455
3514.651912	1170636.078192	42.281460
3514.841545	1170358.890483	42.286464
3514.498940	1170090.738244	42.291469
3514.498986	1169810.250627	42.296474
3514.293357	1169532.518032	42.301479
3514.528103	1169270.738896	42.306484
3514.723452	1168989.797601	42.311488
3514.254030	1168731.221338	42.316493
3514.499454	1168448.355326	42.321498
3514.548020	1168179.096724	42.326503
3514.317846	1167908.454420	42.331508
3514.355828	1167637.565155	42.336512
3514.318216	1167378.473243	42.341517
3514.248614	1167090.960433	42.346522
3514.267103	1166828.339328	42.351527
3514.099487	1166562.053836	42.356532
3514.378684	1166297.380592	42.361536
3513.909592	1166031.117701	42.366541
3513.771288	1165754.778173	42.371546
3514.089925	1165492.512638	42.376551
3513.727408	1165233.934483	42.381556
3513.992929	1164972.312629	42.386560
3514.002670	1164713.458569	42.391565
3513.900514	1164445.826806	42.396570
3513.533714	1164187.197609	42.401575
3513.653443	1163927.908778	42.406580
3514.044174	1163666.673306	42.411584
3513.728795	1163417.821292	42.416589
3514.041113	1163147.787785	42.421594
3514.026714	1162881.667544	42.426599
3513.345231	1162628.681510	42.431604
3513.719809	1162362.470826	42.436608
3513.634685	1162110.589815	42.441613
3513.540684	1161849.910476	42.446618
3513.849188	1161589.907848	42.451623
3513.732130	1161337.333452	42.456628
3513.996012	1161068.051232	42.461632
3513.649288	1160822.199709	42.466637
3513.333091	1160562.816073	42.471642
3513.295112	1160305.925798	42.476647
3513.453348	1160059.293699	42.481652
3513.725350	1159790.795259	42.486656
3513.101210	1159541.242737	42.491661
3513.362852	1159282.551399	42.496666
3513.413022	1159034.754477	42.501671
3513.126354	1158779.059418	42.506676
3513.287625	1158520.630691	42.511680
3513.274193	1158286.424271	42.516685
3513.516166	1158022.851751	42.521690
3513.263299	1157765.021390	42.526695
3513.258674	1157523.687122	42.531700
3513.281963	1157272.123209	42.536704
3513.131764	1157022.656539	42.541709
3512.985975	1156758.327781	42.546714
3512.921040	1156520.362324	42.551719
3512.529508	1156275.345499	42.556724
3512.629810	1156028.155131	42.561728
3512.651888	1155787.588055	42.566733
3512.923442	1155550.847679	42.571738
3512.576888	1155302.466908	42.576743
3512.380992	1155061.713288	42.581748
3512.602235	1154830.530957	42.586752
3512.480917	1154598.164795	42.591757
3513.038251	1154350.157901	42.596762
3512.764233	1154106.061464	42.601767
3512.301420	1153868.609242	42.606772
3512.654019	1153627.510352	42.611776
3512.587977	1153393.189060	42.616781
3512.307557	1153147.345597	42.621786
3512.565512	1152904.052247	42.626791
3512.589836	1152668.264007	42.631796
3512.471418	1152432.488712	42.636800
3512.405917	1152193.096867	42.641805
3512.593867	1151949.865616	42.646810
3512.337952	1151719.571863	42.651815
3512.233369	1151492.935547	42.656820
3512.557293	1151250.785750	42.661824
3512.086316	1151022.769308	42.666829
3512.405168	1150790.919994	42.671834
3512.115240	1150555.562346	42.676839
3512.073728	1150317.122908	42.681844
3512.092754	1150082.166725	42.686848
3512.007821	1149865.022133	42.691853
3512.085948	1149625.584634	42.696858
3512.043828	1149392.975582	42.701863
3511.925275	1149177.039485	42.706868
3512.320392	1148929.751191	42.711872
3512.177435	1148697.791143	42.716877
3511.992512	1148481.648042	42.721882
3512.052170	1148249.255969	42.726887
3511.771859	1148006.203996	42.731892
3512.177112	1147771.365448	42.736896
3511.922976	1147566.849830	42.741901
3511.754663	1147332.086193	42.746906
3511.802428	1147108.552560	42.751911
3511.732860	1146876.310810	42.756916
3511.772975	1146643.756483	42.761920
3511.722341	1146434.519983	42.766925
3511.756917	1146201.852335	42.771930
3511.881805	1145978.921579	42.776935
3511.756129	1145766.258992	42.781940
3511.795142	1145529.485424	42.786945
3511.276961	1145314.120507	42.791949
3511.414396	1145094.752335	42.796954
3511.526742	1144883.626483	42.801959
3511.431714	1144666.079930	42.806964
3511.443696	1144433.622511	42.811969
3511.256105	1144215.314208	42.816973
3511.502202	1144001.760889	42.821978
3511.586423	1143775.994317	42.826983
3511.035335	1143571.562446	42.831988
3511.348693	1143345.739765	42.836993
3511.239168	1143125.951252	42.841997
3511.370312	1142915.786812	42.847002
3511.289408	1142694.837687	42.852007
3511.106370	1142486.320130	42.857012
3511.415977	1142268.797955	42.862017
3511.599697	1142050.623642	42.867021
3511.200441	1141829.785661	42.872026
3511.032539	1141624.835997	42.877031
3511.177522	1141404.175185	42.882036
3511.439462	1141180.355441	42.887041
3511.335958	1140966.167963	42.892045
3511.234958	1140748.840678	42.897050
3511.063665	1140543.470214	42.902055
3511.016798	1140328.203979	42.907060
3511.135767	1140102.464657	42.912065
3511.276220	1139901.097869	42.917069
3511.003425	1139685.937620	42.922074
3510.912058	1139474.629381	42.927079
3510.918593	1139268.421033	42.932084
3511.036602	1139055.258540	42.937089
3510.836150	1138845.651394	42.942093
3510.764617	1138633.736921	42.947098
3511.030897	1138424.605707	42.952103
3510.419052	1138214.756617	42.957108
3510.684439	1137994.218646	42.962113
3510.557505	1137811.610593	42.967117
3510.543673	1137604.201765	42.972122
3510.707287	1137397.515046	42.977127
3510.583378	1137197.892758	42.982132
3510.619542	1136984.090852	42.987137
3510.419868	1136791.301266	42.992141
3510.625516	1136587.993973	42.997146
3510.397840	1136389.212841	43.002151
3510.208478	1136197.159550	43.007156
3510.547136	1135993.522720	43.012161
3510.586678	1135793.250916	43.017165
3510.523775	1135586.910800	43.022170
3510.367751	1135394.728014	43.027175
3510.327485	1135187.134064	43.032180
3510.409839	1134980.556515	43.037185
3510.238777	1134794.147860	43.042189
3509.858469	1134593.045123	43.047194
3510.344231	1134397.491192	43.052199
3510.143912	1134207.647331	43.057204
3510.106581	1134008.365717	43.062209
3510.299634	1133809.418665	43.067213
3510.042998	1133605.123315	43.072218
3510.461066	1133412.679239	43.077223
3510.020662	1133226.734931	43.082228
3510.227609	1133028.326378	43.087233
3510.211734	1132836.122912	43.092237
3509.986415	1132633.780308	43.097242
3509.843693	1132442.058559	43.102247
3509.591280	1132261.465597	43.107252
3509.977036	1132070.213538	43.112257
3509.840867	1131884.267168	43.117261
3509.881614	1131701.801359	43.122266
3509.676073	1131515.948564	43.127271
3509.992692	1131332.284216	43.132276
3510.002513	1131126.994361	43.137281
3509.779275	1130949.963667	43.142285
3509.557366	1130756.198202	43.147290
3509.436427	1130571.058848	43.152295
3509.792938	1130391.727886	43.157300
3509.829689	1130202.557394	43.162305
3509.221664	1130028.506237	43.167309
3509.302497	1129829.143531	43.172314
3509.647343	1129657.014744	43.177319
3509.368604	1129486.219029	43.182324
3509.750032	1129287.452039	43.187329
3509.172492	1129100.910599	43.192333
3509.170368	1128915.028511	43.197338
3509.497186	1128751.240648	43.202343
3509.626742	1128569.984004	43.207348
3509.362415	1128376.043767	43.212353
3509.251962	1128198.902969	43.217357
3509.089997	1128027.185356	43.222362
3509.350259	1127847.118864	43.227367
3509.189725	1127672.251231	43.232372
3509.325482	1127484.869960	43.237377
3509.292274	1127320.241433	43.242381
3509.284836	1127141.431626	43.247386
3509.363523	1126965.930732	43.252391
3509.582441	1126791.257049	43.257396
3509.561029	1126589.126533	43.262401
3509.468535	1126423.053203	43.267405
3509.430182	1126230.234279	43.272410
3509.804953	1126056.271895	43.277415
3508.995722	1125883.830739	43.282420
3509.554101	1125705.164985	43.287425
3509.226357	1125527.495470	43.292429
3508.929929	1125349.814876	43.297434
3509.450949	1125164.286660	43.302439
3508.905397	1124999.956303	43.307444
3509.243196	1124821.487595	43.312449
3509.186966	1124657.066088	43.317453
3509.167589	1124459.707591	43.322458
3508.849136	1124294.461640	43.327463
3508.861990	1124129.727012	43.332468
3508.972422	1123954.216948	43.337473
3508.732072	1123785.135529	43.342477
3508.555152	1123613.183003	43.347482
3508.988467	1123449.309902	43.352487
3508.925148	1123284.181008	43.357492
3508.866240	1123090.776077	43.362497
3508.646137	1122945.651583	43.367501
3509.088189	1122774.426805	43.372506
3508.944872	1122598.342815	43.377511
3508.502687	1122434.106783	43.382516
3508.891459	1122269.348044	43.387521
3508.857422	1122103.035398	43.392525
3508.521582	1121923.247910	43.397530
3508.846755	1121753.437773	43.402535
3508.750840	1121595.497989	43.407540
3508.807916	1121423.626846	43.412545
3508.701244	1121257.775932	43.417549
3508.492161	1121092.031958	43.422554
3508.647545	1120928.889110	43.427559
3508.359541	1120759.719740	43.432564
3508.536304	1120591.992162	43.437569
3508.451523	1120433.540052	43.442573
3508.419542	1120276.217386	43.447578
3508.519743	1120104.106247	43.452583
3508.637843	1119946.749173	43.457588
3508.555160	1119786.753678	43.462593
3508.665249	1119629.102845	43.467597
3508.570673	1119456.050454	43.472602
3508.670451	1119284.579773	43.477607
3508.463021	1119135.634791	43.482612
3508.230471	1118975.353938	43.487617
3508.152937	1118814.756965	43.492621
3508.340675	1118650.681938	43.497626
3508.216047	1118499.609777	43.502631
3508.112013	1118335.001517	43.507636
3508.392718	1118169.753190	43.512641
3508.662756	1118014.124460	43.517645
3508.404474	1117858.482938	43.522650
3508.614001	1117690.182597	43.527655
3508.038232	1117520.958159	43.532660
3508.321965	1117363.878997	43.537665
3508.522523	1117217.672080	43.542669
3508.385295	1117050.361647	43.547674
3508.329510	1116899.995353	43.552679
3508.003060	1116753.100176	43.557684
3508.434586	1116584.728540	43.562689
3508.227504	1116422.175083	43.567693
3508.021885	1116261.331990	43.572698
3508.545811	1116104.748204	43.577703
3507.995690	1115956.533668	43.582708
3508.344728	1115801.590153	43.587713
3508.185031	1115637.575346	43.592717
3508.038087	1115472.886167	43.597722
3508.268314	1115324.906926	43.602727
3508.053511	1115174.709046	43.607732
3508.512969	1115009.810445	43.612737
3507.612789	1114864.006578	43.617741
3507.980587	1114710.077090	43.622746
3508.120103	1114548.077043	43.627751
3507.904100	1114396.427479	43.632756
3508.177601	1114243.072168	43.637761
3508.120225	1114098.062091	43.642765
3507.728476	1113931.363598	43.647770
3508.022919	1113771.793668	43.652775
3507.446032	1113636.010438	43.657780
3507.807831	1113473.178484	43.662785
3507.688704	1113326.536644	43.667789
3507.739509	1113187.396442	43.672794
3508.003272	1113041.923477	43.677799
3507.607530	1112889.784085	43.682804
3507.444501	1112744.564084	43.687809
3507.411865	1112592.165710	43.692813
3507.297589	1112453.224406	43.697818
3507.362089	1112298.894200	43.702823
3506.973622	1112176.300525	43.707828
3507.323208	1112038.512037	43.712833
3507.273955	1111909.656522	43.717837
3507.452799	1111756.436513	43.722842
3507.275944	1111606.323211	43.727847
3507.221262	1111466.392646	43.732852
3507.351309	1111336.730709	43.737857
3507.395563	1111205.553412	43.742861
3507.287788	1111057.416736	43.747866
3507.495314	1110924.202274	43.752871
3507.195038	1110787.061131	43.757876
3507.539014	1110629.965596	43.762881
3507.168351	1110495.118377	43.767885
3507.033905	1110356.316950	43.772890
3507.094351	1110233.318729	43.777895
3506.833171	1110093.863489	43.782900
3507.042790	1109962.056091	43.787905
3507.238700	1109826.812526	43.792909
3507.161323	1109690.847172	43.797914
3507.408890	1109547.667842	43.802919
3507.076726	1109420.898606	43.807924
3506.778008	1109280.092418	43.812929
3506.955574	1109151.705975	43.817933
3506.999737	1109025.247165	43.822938
3507.234639	1108877.375692	43.827943
3506.991887	1108754.489006	43.832948
3507.443068	1108608.006126	43.837953
3507.488256	1108483.920512	43.842957
3506.907057	1108334.736836	43.847962
3507.234599	1108198.285253	43.852967
3506.959282	1108068.802137	43.857972
3507.219120	1107930.254936	43.862977
3507.082564	1107804.465374	43.867981
3507.024108	1107665.677407	43.872986
3506.988709	1107537.096581	43.877991
3507.249045	1107412.187111	43.882996
3507.195410	1107268.710328	43.888001
3506.956982	1107131.752109	43.893005
3506.690063	1106996.418125	43.898010
3507.441063	1106872.274571	43.903015
3506.923989	1106745.663652	43.908020
3507.002779	1106605.011666	43.913025
3507.218581	1106471.685530	43.918029
3507.041079	1106344.149902	43.923034
3507.154087	1106194.506067	43.928039
3506.948132	1106068.209912	43.933044
3507.032522	1105927.252834	43.938049
3507.167986	1105806.719280	43.943053
3506.705513	1105665.749925	43.948058
3506.769002	1105524.403761	43.953063
3506.617458	1105403.335456	43.958068
3506.734124	1105273.338499	43.963073
3506.753691	1105154.050964	43.968077
3506.539149	1105021.141814	43.973082
3507.031936	1104892.410826	43.978087
3506.593177	1104779.303086	43.983092
3506.796169	1104633.326009	43.988097
3506.610618	1104518.642866	43.993101
3506.563790	1104390.370824	43.998106
3506.835311	1104262.902986	44.003111
3506.534296	1104134.093581	44.008116
3506.832712	1104007.092882	44.013121
3506.779829	1103877.854386	44.018125
3506.676041	1103753.779785	44.023130
3506.396883	1103630.782062	44.028135
3505.944809	1103520.516035	44.033140
3506.335519	1103395.969622	44.038145
3506.457013	1103273.375439	44.043149
3506.367782	1103150.144391	44.048154
3506.511108	1103034.706718	44.053159
3506.504363	1102919.960103	44.058164
3506.656272	1102789.228613	44.063169
3506.329968	1102657.521671	44.068173
3506.432139	1102545.233425	44.073178
3506.664102	1102418.492915	44.078183
3506.679619	1102289.969518	44.083188
3506.645260	1102161.451272	44.088193
3506.441228	1102041.080526	44.093197
3506.116010	1101924.740664	44.098202
3506.033407	1101798.993030	44.103207
3506.084297	1101688.511121	44.108212
3506.219437	1101575.337162	44.113217
3506.090371	1101473.863916	44.118221
3505.814389	1101351.291510	44.123226
3506.127824	1101225.082988	44.128231
3505.920251	1101122.182438	44.133236
3505.776799	1101011.431946	44.138241
3506.059917	1100910.549272	44.143245
3505.989301	1100795.098916	44.148250
3506.129125	1100678.751174	44.153255
3505.890137	1100566.860282	44.158260
3505.822432	1100450.924154	44.163265
3505.818000	1100357.534388	44.168269
3505.716033	1100239.209607	44.173274
3505.719190	1100122.872395	44.178279
3505.929270	1100005.733830	44.183284
3505.802322	1099910.540184	44.188289
3505.961941	1099808.032094	44.193293
3506.029282	1099694.543076	44.198298
3506.229176	1099576.154053	44.203303
3505.887106	1099469.324385	44.208308
3505.917690	1099363.769735	44.213313
3505.975350	1099254.479795	44.218317
3505.699322	1099133.291163	44.223322
3506.113719	1099033.690382	44.228327
3505.722697	1098927.431734	44.233332
3505.780410	1098810.866049	44.238337
3505.656523	1098705.802070	44.243341
3505.835343	1098611.491361	44.248346
3506.138477	1098500.233322	44.253351
3505.750829	1098381.341149	44.258356
3505.600942	1098268.240445	44.263361
3505.598845	1098164.771546	44.268365
3505.709210	1098063.290386	44.273370
3505.594452	1097954.863232	44.278375
3505.497233	1097855.516273	44.283380
3505.611675	1097749.820651	44.288385
3505.867407	1097644.960436	44.293389
3505.627163	1097547.735410	44.298394
3505.876500	1097421.161662	44.303399
3506.011218	1097331.522342	44.308404
3505.967072	1097212.930459	44.313409
3505.774567	1097100.290562	44.318413
3505.551702	1096992.435794	44.323418
3505.621664	1096899.834849	44.328423
3505.479535	1096797.223699	44.333428
3505.919886	1096675.957618	44.338433
3505.846489	1096581.079105	44.343437
3505.321753	1096475.272527	44.348442
3505.692283	1096361.663588	44.353447
3505.611970	1096257.310122	44.358452
3505.742806	1096151.963225	44.363457
3505.388560	1096059.991753	44.368461
3505.247724	1095950.189366	44.373466
3505.764169	1095853.957274	44.378471
3505.618853	1095765.007803	44.383476
3505.718443	1095654.011756	44.388481
3505.740973	1095551.828228	44.393485
3505.577337	1095442.880376	44.398490
3505.797961	1095326.117056	44.403495
3505.408034	1095240.452330	44.408500
3505.344764	1095127.941429	44.413505
3505.567441	1095026.384795	44.418509
3505.260245	1094942.615411	44.423514
3505.356724	1094832.081451	44.428519
3505.209003	1094741.871617	44.433524
3505.373126	1094627.303385	44.438529
3505.449429	1094535.235078	44.443533
3505.138056	1094446.674055	44.448538
3505.376233	1094340.604366	44.453543
3505.213417	1094257.566169	44.458548
3505.322356	1094137.637586	44.463553
3505.132775	1094056.227608	44.468557
3505.322443	1093965.757873	44.473562
3505.235560	1093869.398485	44.478567
3504.836707	1093767.824908	44.483572
3505.010495	1093675.247393	44.488577
3505.278764	1093578.537216	44.493581
3504.979167	1093487.182969	44.498586
3505.486198	1093386.888726	44.503591
3505.214815	1093308.065227	44.508596
3505.090645	1093209.977385	44.513601
3505.204638	1093115.102957	44.518605
3505.060255	1093029.649943	44.523610
3505.136459	1092929.226748	44.528615
3504.761390	1092830.216137	44.533620
3505.140593	1092728.973547	44.538625
3505.256851	1092645.386043	44.543629
3505.034093	1092554.386311	44.548634
3505.030121	1092457.030864	44.553639
3505.173197	1092382.529198	44.558644
3505.023714	1092284.524501	44.563649
3504.841551	1092197.437126	44.568653
3504.543046	1092100.506719	44.573658
3505.145955	1092015.872002	44.578663
3504.746216	1091931.018138	44.583668
3505.009717	1091834.660592	44.588673
3505.167265	1091752.297146	44.593677
3504.746465	1091657.485281	44.598682
3505.115175	1091559.382130	44.603687
3504.836941	1091472.298925	44.608692
3504.771374	1091371.774479	44.613697
3504.923701	1091303.863134	44.618701
3504.788697	1091217.613998	44.623706
3505.308443	1091118.328980	44.628711
3504.687334	1091030.337610	44.633716
3504.496356	1090934.038914	44.638721
3504.770344	1090857.771123	44.643725
3505.032256	1090765.129398	44.648730
3505.111077	1090672.516246	44.653735
3504.764967	1090589.164715	44.658740
3505.008211	1090479.666944	44.663745
3505.042185	1090410.518970	44.668749
3504.625118	1090330.335416	44.673754
3504.924935	1090234.230766	44.678759
3504.659869	1090157.946151	44.683764
3504.891637	1090052.751316	44.688769
3504.760296	1089985.157500	44.693773
3504.554436	1089902.251178	44.698778
3504.816831	1089806.911324	44.703783
3505.097679	1089718.941668	44.708788
3505.307312	1089638.453114	44.713793
3505.397328	1089539.018432	44.718797
3504.792370	1089447.167447	44.723802
3504.633501	1089357.827616	44.728807
3504.734247	1089274.190709	44.733812
3504.912412	1089184.792523	44.738817
3504.922264	1089097.240576	44.743821
3504.892573	1089011.705329	44.748826
3504.885439	1088921.758588	44.753831
3504.784768	1088827.323458	44.758836
3505.097052	1088728.028904	44.763841
3504.706989	1088655.671361	44.768845
3504.541737	1088564.882577	44.773850
3504.742186	1088484.570029	44.778855
3504.727022	1088418.566161	44.783860
3504.563553	1088314.935564	44.788865
3504.582465	1088253.235196	44.793869
3504.232382	1088169.368109	44.798874
3504.680001	1088076.649924	44.803879
3504.086177	1087993.778335	44.808884
3504.668494	1087918.089134	44.813889
3504.555880	1087845.675095	44.818893
3504.446882	1087748.156613	44.823898
3504.951612	1087681.100033	44.828903
3504.681048	1087595.486333	44.833908
3504.324722	1087510.939393	44.838913
3504.567429	1087432.999766	44.843917
3504.557080	1087359.700040	44.848922
3504.627000	1087281.882523	44.853927
3504.265865	1087197.427314	44.858932
3504.381161	1087113.658918	44.863937
3504.492611	1087035.064435	44.868941
3504.263603	1086966.299202	44.873946
3504.789433	1086884.280364	44.878951
3504.520071	1086803.062059	44.883956
3504.316560	1086706.786229	44.888961
3504.558710	1086636.885088	44.893965
3504.551342	1086574.115823	44.898970
3504.389054	1086490.287703	44.903975
3504.463865	1086409.965187	44.908980
3504.443037	1086327.357129	44.913985
3504.454906	1086246.563377	44.918989
3504.343431	1086171.443332	44.923994
3504.464108	1086081.811873	44.928999
3504.421886	1086015.591581	44.934004
3504.522286	1085932.478341	44.939009
3504.472619	1085859.548236	44.944013
3504.187314	1085776.975371	44.949018
3504.086364	1085703.572382	44.954023
3503.691252	1085630.696098	44.959028
3504.224586	1085554.311129	44.964033
3504.227285	1085485.776550	44.969037
3503.975849	1085421.883944	44.974042
3504.233128	1085338.544083	44.979047
3503.871792	1085276.968398	44.984052
3504.210051	1085194.571558	44.989057
3504.078909	1085117.523033	44.994061
3504.121867	1085052.427290	44.999066
3503.978990	1084980.075901	45.004071
3503.712108	1084923.561316	45.009076
3503.842718	1084834.578703	45.014081
3504.095242	1084768.582273	45.019085
3504.124426	1084710.291136	45.024090
3503.956079	1084634.008818	45.029095
3504.020671	1084564.589629	45.034100
3504.260042	1084493.990329	45.039105
3504.082734	1084435.538516	45.044109
3503.948685	1084361.260017	45.049114
3504.158922	1084289.991762	45.054119
3503.665220	1084222.577630	45.059124
3503.797274	1084151.032807	45.064129
3504.063673	1084091.161951	45.069133
3503.960092	1084021.092386	45.074138
3503.963280	1083944.292752	45.079143
3503.985721	1083883.788635	45.084148
3504.065414	1083806.207406	45.089153
3503.934244	1083744.576453	45.094157
3503.774644	1083673.361036	45.099162
3504.040191	1083594.499681	45.104167
3503.785508	1083535.859170	45.109172
3503.989556	1083471.676856	45.114177
3504.210213	1083412.093733	45.119181
3503.756135	1083345.812873	45.124186
3503.957402	1083263.601150	45.129191
3503.829813	1083205.703283	45.134196
3503.804876	1083121.800603	45.139201
3503.836199	1083072.697417	45.144205
3503.563724	1083006.670199	45.149210
3503.648617	1082939.528451	45.154215
3503.534557	1082887.954206	45.159220
3504.112446	1082815.359423	45.164225
3504.054228	1082744.594653	45.169229
3503.710063	1082684.808894	45.174234
3503.743944	1082612.205096	45.179239
3503.960045	1082545.132782	45.184244
3504.015929	1082475.496576	45.189249
3503.761399	1082419.241645	45.194253
3503.752030	1082349.039129	45.199258
3504.169150	1082281.259105	45.204263
3503.616555	1082221.310761	45.209268
3503.835863	1082143.491027	45.214273
3503.659737	1082076.381628	45.219277
3503.875622	1082013.235221	45.224282
3503.870763	1081948.302054	45.229287
3503.752161	1081895.760009	45.234292
3503.624407	1081826.337579	45.239297
3503.427842	1081767.956194	45.244301
3503.415222	1081707.913261	45.249306
3503.464975	1081649.202278	45.254311
3503.489427	1081589.247853	45.259316
3503.413227	1081526.431674	45.264321
3503.665590	1081476.702161	45.269325
3503.508065	1081417.063581	45.274330
3503.882396	1081351.964933	45.279335
3503.634606	1081302.508054	45.284340
3503.614107	1081230.854065	45.289345
3503.728259	1081168.769833	45.294349
3503.459924	1081106.939748	45.299354
3503.983306	1081035.481406	45.304359
3503.828368	1080985.334837	45.309364
3503.991579	1080914.989487	45.314369
3503.478605	1080852.909008	45.319373
3503.601179	1080783.623930	45.324378
3503.591554	1080718.389084	45.329383
3503.480973	1080671.686039	45.334388
3503.219353	1080612.439543	45.339393
3503.405528	1080562.904475	45.344397
3503.255797	1080497.018478	45.349402
3503.282391	1080436.763199	45.354407
3503.157389	1080385.742706	45.359412
3503.151499	1080347.558513	45.364417
3503.185457	1080285.957150	45.369421
3503.482291	1080229.684733	45.374426
3503.581354	1080162.986162	45.379431
3503.224831	1080125.529785	45.384436
3503.290785	1080057.971858	45.389441
3503.604342	1080006.779641	45.394445
3503.637820	1079944.598808	45.399450
3503.621293	1079886.551406	45.404455
3503.226782	1079832.403727	45.409460
3503.436588	1079770.287818	45.414465
3503.549662	1079710.490038	45.419469
3503.412402	1079662.343421	45.424474
3503.579458	1079605.798078	45.429479
3502.996268	1079545.441464	45.434484
3502.967332	1079477.412187	45.439489
3503.290324	1079439.071509	45.444493
3503.107559	1079397.071423	45.449498
3503.252008	1079331.602687	45.454503
3503.186323	1079273.460894	45.459508
3503.156610	1079225.580593	45.464513
3503.312299	1079175.462171	45.469517
3503.305272	1079130.168318	45.474522
3503.436194	1079062.299465	45.479527
3503.165507	1079010.906233	45.484532
3503.166851	1078957.836265	45.489537
3503.292417	1078907.240504	45.494541
3503.003124	1078854.601271	45.499546
3503.169852	1078804.765536	45.504551
3502.969788	1078759.212483	45.509556
3503.113289	1078709.571646	45.514561
3503.258044	1078649.852995	45.519565
3502.933800	1078611.901024	45.524570
3503.329558	1078551.948017	45.529575
3502.938017	1078513.910472	45.534580
3503.236461	1078457.811473	45.539585
3503.434193	1078416.604956	45.544589
3502.905157	1078357.282003	45.549594
3503.317079	1078295.403954	45.554599
3503.031912	1078246.981260	45.559604
3503.064088	1078205.416494	45.564609
3503.097650	1078148.014205	45.569613
3503.029367	1078096.099104	45.574618
3503.570646	1078037.748194	45.579623
3502.754369	1078005.440090	45.584628
3503.065969	1077955.572743	45.589633
3503.271541	1077898.235484	45.594637
3502.949950	1077848.087493	45.599642
3503.025685	1077804.304795	45.604647
3503.389267	1077762.682078	45.609652
3503.364157	1077695.397857	45.614657
3503.110940	1077650.900187	45.619661
3503.547358	1077601.297023	45.624666
3503.051140	1077538.696045	45.629671
3503.204044	1077496.722030	45.634676
3502.770793	1077442.077009	45.639681
3503.359091	1077393.598877	45.644685
3502.991877	1077345.853658	45.649690
3502.963653	1077292.772367	45.654695
3502.796502	1077254.593078	45.659700
3502.778902	1077206.021075	45.664705
3503.026626	1077165.276876	45.669709
3502.743970	1077127.115718	45.674714
3502.962703	1077068.807586	45.679719
3502.734172	1077029.100815	45.684724
3502.684406	1076999.828544	45.689729
3502.700794	1076942.608412	45.694733
3502.714426	1076894.796520	45.699738
3503.052530	1076858.739339	45.704743
3503.101557	1076829.257874	45.709748
3503.082888	1076767.913468	45.714753
3502.966213	1076723.577757	45.719757
3503.200968	1076678.607762	45.724762
3503.405053	1076615.016777	45.729767
3503.059651	1076577.726188	45.734772
3503.236692	1076527.963985	45.739777
3502.966421	1076480.195221	45.744781
3502.991736	1076429.400986	45.749786
3503.065858	1076379.558369	45.754791
3503.161646	1076339.409114	45.759796
3503.362119	1076269.189755	45.764801
3503.137674	1076223.619540	45.769805
3503.161557	1076173.687304	45.774810
3503.082914	1076103.127713	45.779815
3503.067753	1075998.853974	45.784820
3502.866277	1075833.442926	45.789825
3503.091344	1075597.089393	45.794829
3503.033914	1075309.587493	45.799834
3502.939227	1074970.600647	45.804839
3502.624050	1074549.319068	45.809844
3502.455099	1074068.716226	45.814849
3502.633200	1073525.093025	45.819853
3502.514971	1072930.353723	45.824858
3502.845377	1072255.725600	45.829863
3502.792673	1071520.824135	45.834868
3502.580123	1070701.367967	45.839873
3502.791125	1069834.136324	45.844877
3502.196938	1068885.466226	45.849882
3501.990738	1067854.926569	45.854887
3502.020224	1066763.944990	45.859892
3501.899333	1065595.329016	45.864897
3501.998804	1064349.256834	45.869901
3501.460169	1063016.866349	45.874906
3501.408497	1061618.126788	45.879911
3501.085152	1060147.623875	45.884916
3500.955946	1058580.853515	45.889921
3500.727510	1056953.818600	45.894925
3500.237481	1055232.566082	45.899930
3499.950841	1053430.140557	45.904935
3499.666407	1051567.811262	45.909940
3499.449697	1049597.652772	45.914945
3499.107385	1047572.860250	45.919949
3498.845435	1045450.857088	45.924954
3498.829989	1043244.158940	45.929959
3498.458013	1040965.134216	45.934964
3497.974766	1038592.773285	45.939969
3497.810628	1036146.714019	45.944973
3497.418327	1033611.759777	45.949978
3496.818965	1030981.785551	45.954983
3496.439699	1028308.114045	45.959988
3496.071689	1025518.335044	45.964993
3496.097484	1022657.102113	45.969997
3495.252083	1019706.474640	45.975002
3494.882976	1016681.717763	45.980007
3494.517420	1013583.278280	45.985012
3493.955964	1010379.493003	45.990017
3493.666165	1007100.635336	45.995021
3493.051887	1003764.769846	46.000026
3492.672783	1000314.279893	46.005031
3491.880123	996783.837560	46.010036
3491.397818	993167.428862	46.015041
3490.871873	989474.315101	46.020045
3490.110811	985706.237964	46.025050
3489.488426	981848.442750	46.030055
3489.203228	977909.124894	46.035060
3488.274001	973900.409863	46.040065
3487.923742	969809.040077	46.045069
3487.304182	965624.899339	46.050074
3486.823137	961352.919695	46.055079
3485.843154	957001.355451	46.060084
3485.234137	952621.371327	46.065089
3484.701539	948216.246178	46.070093
3483.907485	943724.504855	46.075098
3483.018321	939153.699418	46.080103
3482.193838	934512.465460	46.085108
3481.436063	929777.789392	46.090113
3480.916603	924962.609795	46.095117
3479.968658	920068.788621	46.100122
3479.133453	915079.787393	46.105127
3477.884356	910018.526897	46.110132
3477.039734	904870.824658	46.115137
3476.443901	899654.198371	46.120141
3475.410417	894356.246291	46.125146
3474.262976	888952.643429	46.130151
3473.203355	883490.007594	46.135156
3472.269900	877934.092927	46.140161
3471.657794	872313.687989	46.145165
3470.326944	866598.728285	46.150170
3469.628898	860786.941334	46.155175
3468.543142	854911.774283	46.160180
3467.232341	848949.025194	46.165185
3466.052327	842879.490120	46.170189
3464.388023	836761.321522	46.175194
3463.737564	830538.466628	46.180199
3462.980193	824262.437969	46.185204
3461.705688	817877.137644	46.190209
3460.907579	811399.864536	46.195213
3459.503977	804861.326882	46.200218
3458.195057	798228.583093	46.205223
3456.912772	791514.886842	46.210228
3455.842527	784709.501460	46.215233
3454.810894	777814.808355	46.220237
3453.234049	770849.039033	46.225242
3452.213704	763796.283666	46.230247
3450.529242	756673.989838	46.235252
3449.141860	749454.986320	46.240257
3448.216576	742159.671869	46.245261
3446.666758	734793.086812	46.250266
3445.162367	727305.394631	46.255271
3443.629295	719755.974231	46.260276
3442.253191	712126.787729	46.265281
3440.948756	704427.856175	46.270285
3439.103322	696632.873437	46.275290
3437.800216	688754.589648	46.280295
3436.408590	680820.686156	46.285300
3434.689619	672781.592074	46.290305
3433.161714	664673.784430	46.295309
3431.603490	656492.435974	46.300314
3429.841053	648208.806049	46.305319
3427.818618	639864.038104	46.310324
3426.429723	631449.790352	46.315329
3425.124676	622949.018285	46.320333
3422.770652	614382.136907	46.325338
3421.361099	605722.842851	46.330343
3419.241201	597005.832317	46.335348
3417.580323	588228.051010	46.340353
3415.693098	579339.265543	46.345357
3413.596720	570389.859060	46.350362
3411.881677	561380.153349	46.355367
3410.051302	552293.670493	46.360372
3407.827870	543125.660763	46.365377
3406.117851	533895.298592	46.370381
3403.671316	524589.547381	46.375386
3401.464384	515225.447992	46.380391
3399.662486	505790.190574	46.385396
3397.665739	496279.972149	46.390401
3395.758672	486705.522102	46.395405
3393.146726	477067.751460	46.400410
3391.132192	467348.233729	46.405415
3388.676415	457579.745861	46.410420
3386.321202	447751.156563	46.415425
3384.063152	437843.139791	46.420429
3381.477402	427895.956966	46.425434
3378.871106	417860.827925	46.430439
3376.602942	407778.483017	46.435444
3373.931513	397647.291420	46.440449
3371.388074	387449.377606	46.445453
3368.397191	377220.096667	46.450458
3366.033955	366912.559349	46.455463
3363.476085	356568.598235	46.460468
3360.450097	346182.320694	46.465473
3357.721872	335742.114761	46.470477
3354.293015	325242.588036	46.475482
3351.637677	314702.207867	46.480487
3348.557031	304144.483787	46.485492
3345.301888	293525.270987	46.490497
3342.395843	282876.667763	46.495501
3338.734510	272190.282265	46.500506
3335.693380	261470.536202	46.505511
3332.221498	250708.046006	46.510516
3329.037479	239917.311829	46.515521
3325.531929	229077.812148	46.520525
3321.618397	218200.373357	46.525530
3317.986035	207348.678530	46.530535
3314.058850	196478.464025	46.535540
3310.286500	185589.470399	46.540545
3306.515955	174706.477950	46.545549
3301.903365	163801.497977	46.550554
3297.636679	152897.966548	46.555559
3292.899858	141999.273747	46.560564
3288.312484	131105.684693	46.565569
3283.718504	120231.146599	46.570573
3278.222663	109373.516356	46.575578
3273.057789	98536.546942	46.580583
3267.096032	87745.274497	46.585588
3261.347135	77007.587586	46.590593
3254.718490	66301.563288	46.595597
3246.734424	55677.997456	46.600602
3238.046036	45173.694506	46.605607
3219.948244	35045.606836	46.610612
3180.534329	25673.938407	46.615617
3128.672270	17095.510767	46.620621
3070.061826	9472.172008	46.625626
3011.289765	2816.519513	46.630631
2841.683309	434.251557	46.635636
2662.712043	437.970702	46.640641
2594.949935	430.862217	46.645645
2619.773733	420.064657	46.650650
2695.447734	399.207189	46.655655
2776.572777	375.838324	46.660660
2836.777723	371.749617	46.665665
2868.311337	376.249943	46.670669
2875.210414	386.084118	46.675674
2868.164982	399.488352	46.680679
2856.199867	391.230082	46.685684
2844.123871	375.220077	46.690689
2835.962908	369.672345	46.695693
2831.186218	368.889229	46.700698
2829.027427	376.994304	46.705703
2827.960478	370.808282	46.710708
2827.088958	361.830968	46.715713
2825.926110	364.053620	46.720717
2823.477904	355.215773	46.725722
2820.574858	353.005594	46.730727
2817.235752	367.002069	46.735732
2814.066169	365.065902	46.740737
2811.699346	357.215530	46.745741
2808.214920	354.374089	46.750746
2805.051138	344.360025	46.755751
2801.755982	346.570550	46.760756
2798.308549	359.401280	46.765761
2795.934123	353.135536	46.770765
2792.620324	342.098166	46.775770
2789.429795	351.078337	46.780775
2786.055143	339.698499	46.785780
2782.750951	348.786991	46.790785
2779.636286	344.546211	46.795789
2776.496177	346.948035	46.800794
2773.523950	342.824067	46.805799
2770.002567	344.584135	46.810804
2766.438477	336.467087	46.815809
2763.583122	330.189393	46.820813
2760.049653	341.933677	46.825818
2756.894861	340.766802	46.830823
2753.405314	333.713834	46.835828
2750.025919	332.266807	46.840833
2746.835269	333.081969	46.845837
2742.975205	332.996843	46.850842
2739.526117	336.289791	46.855847
2736.398322	329.629441	46.860852
2733.228600	333.491564	46.865857
2730.027270	316.174279	46.870861
2726.324463	323.600205	46.875866
2723.417836	326.764162	46.880871
2719.356455	319.637579	46.885876
2716.201377	320.403183	46.890881
2712.959467	324.749488	46.895885
2709.273382	317.562616	46.900890
2706.327044	319.772888	46.905895
2702.790131	322.258607	46.910900
2699.274868	328.882812	46.915905
2695.818694	313.588222	46.920909
2691.898687	323.761089	46.925914
2688.709085	308.872734	46.930919
2685.703229	320.111236	46.935924
2682.209448	327.927243	46.940929
2679.098758	319.001386	46.945933
2675.009111	318.313561	46.950938
2671.682524	318.622656	46.955943
2668.725409	319.213276	46.960948
2664.936006	320.407674	46.965953
2661.614649	311.111377	46.970957
2657.766759	318.868074	46.975962
2653.885619	310.595208	46.980967
2651.312774	309.120120	46.985972
2647.896678	314.734703	46.990977
2644.904000	306.486627	46.995981
2641.157806	316.426433	47.000986
2637.702581	310.374285	47.005991
2633.410910	308.539451	47.010996
2629.871474	303.096298	47.016001
2627.128612	297.375403	47.021005
2623.722822	305.225157	47.026010
2619.820494	295.871466	47.031015
2616.264714	295.944599	47.036020
2612.662204	308.034246	47.041025
2609.526209	300.068501	47.046029
2606.171660	303.590581	47.051034
2603.032349	284.265661	47.056039
2599.682553	292.114373	47.061044
2596.527958	297.245050	47.066049
2592.735366	288.407222	47.071053
2588.769149	297.661141	47.076058
2585.448520	296.567957	47.081063
2582.012347	291.887202	47.086068
2578.323949	294.624762	47.091073
2575.088288	286.063602	47.096077
2571.687303	290.875404	47.101082
2568.026105	290.087396	47.106087
2564.457598	293.552129	47.111092
2561.395058	292.993844	47.116097
2557.903345	278.571250	47.121101
2554.111026	287.270857	47.126106
2550.956580	295.343295	47.131111
2546.988269	293.354564	47.136116
2543.339136	281.573147	47.141121
2540.584349	282.348585	47.146125
2536.593914	287.857038	47.151130
2533.368468	283.299020	47.156135
2529.990104	289.581740	47.161140
2526.494214	292.822304	47.166145
2523.122275	277.637092	47.171149
2518.939424	286.378318	47.176154
2515.894278	293.652955	47.181159
2512.452349	279.246745	47.186164
2509.103338	287.907406	47.191169
2506.325785	287.123087	47.196173
2502.176951	283.549324	47.201178
2498.401661	284.663139	47.206183
2495.028689	285.257876	47.211188
2491.336047	275.577082	47.216193
2488.123839	281.874741	47.221197
2483.881047	297.976542	47.226202
2481.220002	283.172443	47.231207
2477.683083	285.090975	47.236212
2474.216688	299.890041	47.241217
2470.623076	273.945924	47.246221
2466.989647	275.528266	47.251226
2463.226289	277.777452	47.256231
2460.284024	285.079039	47.261236
2456.511560	279.850022	47.266241
2453.493505	274.902087	47.271245
2449.749759	279.448635	47.276250
2446.611247	275.156019	47.281255
2442.955878	278.666104	47.286260
2439.045815	283.737120	47.291265
2435.790447	268.355065	47.296269
2431.667888	268.150599	47.301274
2428.409599	267.679601	47.306279
2425.184776	268.285356	47.311284
2422.012729	273.607401	47.316289
2418.305034	257.775792	47.321293
2414.774085	270.658522	47.326298
2411.662000	272.819866	47.331303
2408.025967	268.067982	47.336308
2404.283158	270.852179	47.341313
2401.019833	260.090795	47.346317
2397.704327	271.681110	47.351322
2394.121852	267.367319	47.356327
2390.490874	258.544709	47.361332
2386.640375	274.819199	47.366337
2383.464389	253.546892	47.371341
2379.429921	272.442457	47.376346
2376.344067	270.980643	47.381351
2373.097455	261.388960	47.386356
2369.473867	270.174755	47.391361
2366.022915	273.313952	47.396365
2362.382818	259.200001	47.401370
2359.183815	268.156996	47.406375
2355.813054	260.731096	47.411380
2351.683687	267.891764	47.416385
2348.781244	254.334050	47.421389
2345.332657	265.154305	47.426394
2341.278922	269.358477	47.431399
2337.860503	267.075056	47.436404
2334.365497	266.402118	47.441409
2331.156224	265.072951	47.446413
2327.593083	260.267161	47.451418
2324.147646	257.667766	47.456423
2320.584199	262.435320	47.461428
2316.725477	264.248352	47.466433
2313.310201	246.620396	47.471437
2309.949219	259.390768	47.476442
2306.652107	254.354262	47.481447
2302.934116	259.829030	47.486452
2299.203479	258.013749	47.491457
2295.969096	254.905612	47.496461
2292.968940	261.058259	47.501466
2289.596369	257.117163	47.506471
2285.823898	250.098318	47.511476
2282.032988	256.963852	47.516481
2278.454536	251.664569	47.521485
2274.870344	257.109291	47.526490
2271.579129	256.457528	47.531495
2268.056778	256.653762	47.536500
2264.528417	254.558792	47.541505
2261.240619	256.775317	47.546509
2257.632727	258.146264	47.551514
2254.122977	250.574742	47.556519
2250.382769	256.469726	47.561524
2247.132096	261.018995	47.566529
2243.624536	248.646962	47.571533
2240.073169	253.203896	47.576538
2236.581133	242.605531	47.581543
2233.340622	249.766350	47.586548
2229.547760	252.285009	47.591553
2226.229804	248.830394	47.596557
2222.574216	239.869195	47.601562
2218.869214	243.720822	47.606567
2215.543763	247.943053	47.611572
2212.202178	251.607478	47.616577
2208.593344	246.442486	47.621581
2204.953008	254.633238	47.626586
2201.586341	250.453253	47.631591
2198.227617	248.736509	47.636596
2194.741581	255.154898	47.641601
2191.150136	248.837200	47.646605
2187.916448	253.563343	47.651610
2184.319603	257.971925	47.656615
2180.720658	253.608874	47.661620
2176.925422	241.023093	47.666625
2173.327078	253.686444	47.671629
2169.659293	253.115780	47.676634
2166.656617	247.526545	47.681639
2163.112931	251.392337	47.686644
2159.793573	243.913479	47.691649
2156.434717	250.329255	47.696653
2152.597024	245.451347	47.701658
2149.270329	241.767356	47.706663
2146.158573	251.288051	47.711668
2142.139597	255.689128	47.716673
2138.941398	242.798010	47.721677
2135.065389	254.122624	47.726682
2131.725489	251.421268	47.731687
2128.155140	250.489254	47.736692
2124.517555	251.617829	47.741697
2121.107187	246.268019	47.746701
2117.714813	250.801246	47.751706
2114.314470	243.557353	47.756711
2110.593265	245.430280	47.761716
2106.916639	250.492829	47.766721
2103.497322	228.975560	47.771725
2100.068434	247.940890	47.776730
2096.960650	248.800560	47.781735
2093.330318	240.020646	47.786740
2089.721550	239.848233	47.791745
2086.281752	234.919237	47.796749
2082.834826	243.110390	47.801754
2079.209747	240.741812	47.806759
2075.498569	231.919607	47.811764
2071.972224	241.324811	47.816769
2068.675590	239.562666	47.821773
2064.817290	237.380847	47.826778
2061.646578	241.952115	47.831783
2058.273296	243.659253	47.836788
2054.493580	234.988259	47.841793
2051.364376	235.121717	47.846797
2047.914254	238.093684	47.851802
2044.680533	231.741533	47.856807
2040.808562	231.699083	47.861812
2036.498085	244.653285	47.866817
2033.189616	239.254059	47.871821
2029.890832	230.468431	47.876826
2027.083271	229.741733	47.881831
2023.923639	240.774871	47.886836
2020.056776	240.681274	47.891841
2016.657197	236.759967	47.896845
2012.744834	248.510112	47.901850
2009.079131	232.504554	47.906855
2005.405757	222.653486	47.911860
2001.654170	246.606281	47.916865
1998.857843	224.370902	47.921869
1995.308135	238.948799	47.926874
1991.824372	220.734126	47.931879
1988.241932	234.339144	47.936884
1984.466388	241.191611	47.941889
1981.046725	221.596819	47.946893
1977.500078	237.711186	47.951898
1974.022288	243.409487	47.956903
1970.723143	237.492387	47.961908
1967.100507	243.381612	47.966913
1963.900575	245.154609	47.971917
1960.413652	223.731767	47.976922
1956.632735	230.850811	47.981927
1953.493791	234.173213	47.986932
1949.369825	242.770300	47.991937
1946.244708	231.147414	47.996941
1942.829007	227.474560	48.001946
1939.099040	225.627792	48.006951
1935.831624	230.809857	48.011956
1931.928896	236.839321	48.016961
1928.643209	223.344394	48.021965
1925.154074	241.073572	48.026970
1921.732055	237.985915	48.031975
1918.317536	232.882654	48.036980
1914.262329	237.114997	48.041985
1911.173873	230.845992	48.046989
1907.757575	232.288690	48.051994
1904.525163	225.049279	48.056999
1900.670327	229.369722	48.062004
1897.116126	237.656579	48.067009
1893.543820	231.662548	48.072013
1890.173070	231.530286	48.077018
1886.684026	233.389487	48.082023
1883.327189	230.445099	48.087028
1879.588979	231.228915	48.092033
1876.407052	225.039280	48.097037
1872.505543	232.775127	48.102042
1869.146684	226.841200	48.107047
1865.928266	218.024060	48.112052
1861.772917	228.629575	48.117057
1858.489096	226.722365	48.122061
1854.967165	226.845622	48.127066
1851.692977	226.661832	48.132071
1848.593013	233.477384	48.137076
1844.703883	229.707375	48.142081
1841.660218	219.353453	48.147085
1837.556771	232.055547	48.152090
1833.949471	221.034669	48.157095
1830.307735	220.090708	48.162100
1826.988933	226.154303	48.167105
1823.635159	211.489865	48.172109
1820.125920	225.477975	48.177114
1816.723031	221.794688	48.182119
1813.168838	218.256135	48.187124
1809.242031	225.194007	48.192129
1806.119240	220.992147	48.197133
1802.773156	226.024559	48.202138
1799.138632	220.336622	48.207143
1795.892086	223.211476	48.212148
1791.990136	218.745721	48.217153
1788.939045	211.708698	48.222157
1785.268532	225.805805	48.227162
1781.828672	230.106575	48.232167
1778.179982	219.103709	48.237172
1774.150212	221.178752	48.242177
1771.268192	212.631630	48.247181
1767.357387	211.936020	48.252186
1764.020240	215.374166	48.257191
1760.693246	224.757341	48.262196
1757.220745	226.151370	48.267201
1753.646507	215.464863	48.272205
1749.830373	209.295588	48.277210
1746.473332	215.956964	48.282215
1743.338782	218.210177	48.287220
1739.868222	215.949274	48.292225
1735.947639	220.676747	48.297229
1732.027719	226.035613	48.302234
1728.980663	220.015588	48.307239
1725.907567	208.690882	48.312244
1722.195613	220.534338	48.317249
1718.711197	211.736310	48.322253
1714.946826	213.241262	48.327258
1711.451442	227.868783	48.332263
1708.201857	218.177745	48.337268
1704.150976	210.419404	48.342273
1701.040235	221.006728	48.347277
1697.539301	219.498573	48.352282
1694.092844	215.265033	48.357287
1690.730951	210.731441	48.362292
1686.966908	222.224793	48.367297
1683.536879	206.749152	48.372301
1679.981242	220.612860	48.377306
1676.445174	223.612094	48.382311
1673.290266	215.454357	48.387316
1669.424949	219.412598	48.392321
1666.135162	213.387278	48.397325
1662.450904	202.598234	48.402330
1658.940645	217.231967	48.407335
1655.462769	218.973805	48.412340
1652.264905	215.593585	48.417345
1648.567144	200.208915	48.422349
1645.009871	219.380892	48.427354
1641.775699	219.122326	48.432359
1638.299355	208.607483	48.437364
1634.277482	212.255749	48.442369
1630.740253	208.418035	48.447373
1627.260910	209.305768	48.452378
1623.988663	216.724197	48.457383
1620.333275	210.338167	48.462388
1617.024118	219.145650	48.467393
1613.709333	216.380132	48.472397
1610.463324	222.652197	48.477402
1606.842793	213.922469	48.482407
1602.926391	210.764729	48.487412
1599.150469	218.673929	48.492417
1596.009984	209.068348	48.497421
1592.312597	217.957663	48.502426
1589.037030	215.683010	48.507431
1585.913945	215.794152	48.512436
1581.775295	210.393455	48.517441
1578.339673	207.166159	48.522445
1574.883919	207.780594	48.527450
1571.137920	207.021986	48.532455
1567.927658	207.504558	48.537460
1564.051677	212.827148	48.542465
1561.349241	213.285016	48.547469
1557.905168	217.921414	48.552474
1553.896787	210.179440	48.557479
1550.579483	197.766022	48.562484
1547.141941	206.101727	48.567489
1543.756461	202.552352	48.572493
1539.758304	217.654653	48.577498
1536.249415	205.328100	48.582503
1533.327952	197.730370	48.587508
1529.275510	211.318973	48.592513
1526.088547	201.305074	48.597517
1522.158650	199.612776	48.602522
1518.767256	204.638767	48.607527
1515.539102	209.416339	48.612532
1511.712273	209.263728	48.617537
1508.625738	200.232156	48.622541
1504.984827	203.275110	48.627546
1501.437227	194.541710	48.632551
1498.022247	202.992689	48.637556
1494.317071	209.557120	48.642561
1491.160684	184.420976	48.647565
1487.300220	197.671183	48.652570
1483.667028	212.441968	48.657575
1480.612832	202.741020	48.662580
1476.887544	209.277505	48.667585
1473.599923	204.389632	48.672589
1469.604113	209.762034	48.677594
1466.108587	193.431554	48.682599
1462.818325	197.395520	48.687604
1459.193694	203.461779	48.692609
1455.934494	192.474374	48.697613
1452.125098	205.011180	48.702618
1448.510145	204.455452	48.707623
1445.255113	195.019515	48.712628
1442.310679	205.343086	48.717633
1438.859516	199.167438	48.722637
1435.221061	200.849656	48.727642
1431.437199	198.730497	48.732647
1427.848369	199.840119	48.737652
1423.717622	210.908113	48.742657
1420.999682	192.099646	48.747661
1417.473687	201.477005	48.752666
1413.958201	195.760971	48.757671
1410.405885	191.755296	48.762676
1406.472467	193.590291	48.767681
1403.296416	190.945431	48.772685
1399.668868	197.975964	48.777690
1396.264058	195.728166	48.782695
1393.236897	204.876999	48.787700
1389.158212	192.567246	48.792705
1385.808475	189.447720	48.797709
1382.309573	196.642204	48.802714
1378.943963	196.008365	48.807719
1375.267517	193.866774	48.812724
1371.513058	199.171469	48.817729
1368.531794	203.338122	48.822733
1364.895498	205.582949	48.827738
1361.227736	203.806930	48.832743
1358.103596	199.929304	48.837748
1354.127771	201.517388	48.842753
1350.331157	194.178931	48.847757
1347.110892	198.308579	48.852762
1343.658401	205.035293	48.857767
1340.724008	193.138013	48.862772
1336.942717	210.901249	48.867777
1333.563301	204.634891	48.872781
1329.890444	205.905921	48.877786
1326.217851	208.902398	48.882791
1323.023198	189.619908	48.887796
1319.192909	192.289721	48.892801
1316.111682	195.417474	48.897805
1312.408822	195.768372	48.902810
1308.473881	193.436361	48.907815
1304.904709	183.118390	48.912820
1301.008397	189.676962	48.917825
1297.994775	193.491452	48.922829
1294.380874	194.801998	48.927834
1291.208430	200.551792	48.932839
1287.784643	184.372975	48.937844
1284.531906	194.054026	48.942849
1281.280151	196.778323	48.947853
1277.227573	191.233201	48.952858
1273.671334	198.095157	48.957863
1270.493458	199.903579	48.962868
1266.337671	193.595725	48.967873
1263.295347	194.751268	48.972877
1259.974594	200.416343	48.977882
1256.219180	196.508106	48.982887
1252.694574	182.559095	48.987892
1248.848015	185.576529	48.992897
1245.447805	191.502348	48.997901
1242.364799	193.479706	49.002906
1238.707707	176.015189	49.007911
1235.418192	184.714093	49.012916
1231.590360	197.593895	49.017921
1228.312651	191.499540	49.022925
1224.947065	188.544015	49.027930
1221.200269	202.394043	49.032935
1217.645473	178.234957	49.037940
1214.012298	200.003946	49.042945
1211.092365	195.367665	49.047949
1207.213766	193.217214	49.052954
1203.404302	185.776400	49.057959
1200.204333	196.298591	49.062964
1196.359999	198.208970	49.067969
1193.259018	179.434880	49.072973
1189.539975	203.749650	49.077978
1186.058724	190.169496	49.082983
1182.850445	181.071590	49.087988
1178.948513	185.822500	49.092993
1175.919711	199.717788	49.097997
1172.247921	193.623799	49.103002
1168.747385	201.000171	49.108007
1165.065314	188.573811	49.113012
1161.141431	189.505754	49.118017
1158.074296	191.921321	49.123021
1154.639217	198.719230	49.128026
1151.111187	193.230450	49.133031
1147.937514	187.611159	49.138036
1144.092359	193.994144	49.143041
1140.691478	177.465963	49.148045
1136.908174	181.298363	49.153050
1133.385751	186.271661	49.158055
1130.325609	187.663424	49.163060
1126.205188	189.097431	49.168065
1122.951064	176.421501	49.173069
1119.760984	193.362868	49.178074
1116.439620	185.308695	49.183079
1112.726046	185.801164	49.188084
1109.198758	181.489150	49.193089
1105.822490	192.075202	49.198093
1102.146008	192.697402	49.203098
1098.335845	177.639104	49.208103
1095.202897	182.209142	49.213108
1091.297305	184.538320	49.218113
1087.898789	186.548593	49.223117
1084.518360	189.810383	49.228122
1080.872996	181.917649	49.233127
1077.785311	185.136341	49.238132
1073.743813	197.609902	49.243137
1070.580514	183.745301	49.248141
1067.198954	191.067838	49.253146
1063.515393	191.393880	49.258151
1060.003499	186.304216	49.263156
1056.407866	195.754185	49.268161
1053.102752	190.444124	49.273165
1049.735705	181.584909	49.278170
1046.003238	186.910200	49.283175
1042.434365	183.827427	49.288180
1038.622887	185.646438	49.293185
1035.905435	165.428568	49.298189
1032.054962	171.696854	49.303194
1028.332064	185.360289	49.308199
1024.640466	175.036372	49.313204
1021.017216	185.030751	49.318209
1017.848476	185.175238	49.323213
1014.645208	173.470726	49.328218
1011.092859	183.214065	49.333223
1008.058912	186.688803	49.338228
1004.336275	186.642492	49.343233
1000.626691	179.722301	49.348237
997.143259	188.626948	49.353242
993.145174	192.119304	49.358247
989.750110	179.352678	49.363252
986.093915	184.542482	49.368257
983.123630	177.025414	49.373261
979.967998	181.646895	49.378266
976.142768	175.297791	49.383271
972.766052	185.954108	49.388276
968.365507	186.838680	49.393281
964.919362	182.811485	49.398285
961.889880	180.794656	49.403290
958.154161	171.246988	49.408295
955.187787	176.682310	49.413300
951.665944	196.500040	49.418305
947.984448	181.887538	49.423309
944.208480	181.923761	49.428314
941.139948	181.736536	49.433319
937.702166	180.145942	49.438324
933.854875	186.340555	49.443329
930.335862	181.130303	49.448333
926.550679	182.677185	49.453338
923.216745	179.445885	49.458343
920.048953	174.770666	49.463348
916.344171	181.088062	49.468353
913.063445	173.877314	49.473357
909.700687	181.996013	49.478362
906.006733	187.584047	49.483367
902.645617	185.460208	49.488372
898.854399	183.145065	49.493377
895.245899	180.297206	49.498381
891.818451	182.318072	49.503386
888.244026	185.432826	49.508391
884.784860	184.772359	49.513396
881.087821	177.421910	49.518401
877.759363	166.147181	49.523405
874.679865	177.730645	49.528410
871.089474	182.340990	49.533415
867.538217	173.724315	49.538420
863.656941	188.485364	49.543425
860.155405	179.156083	49.548429
856.568351	176.424867	49.553434
853.292146	184.854269	49.558439
850.138787	174.027142	49.563444
846.348918	182.780897	49.568449
843.180885	190.196028	49.573453
839.297722	182.757556	49.578458
836.136920	180.855206	49.583463
832.338652	171.138594	49.588468
828.488891	181.891427	49.593473
825.155366	177.228233	49.598477
822.068730	173.542789	49.603482
818.282533	184.874101	49.608487
814.904512	169.366810	49.613492
811.008641	179.234337	49.618497
807.716627	177.555813	49.623501
803.912444	187.369338	49.628506
800.559166	183.944184	49.633511
797.693697	177.825801	49.638516
793.942736	185.390088	49.643521
790.670807	176.812275	49.648525
786.555531	178.931088	49.653530
783.277329	192.513303	49.658535
780.002084	184.361538	49.663540
776.010296	192.002009	49.668545
773.122010	182.516067	49.673549
769.542167	181.818960	49.678554
765.531928	170.237107	49.683559
761.976705	170.694640	49.688564
758.324033	190.917402	49.693569
755.064778	183.009748	49.698573
751.708277	177.046566	49.703578
747.886308	182.556964	49.708583
744.707759	173.739122	49.713588
741.162025	183.257042	49.718593
738.037553	190.637102	49.723597
734.698311	180.853428	49.728602
730.855430	182.160349	49.733607
727.574751	173.928621	49.738612
723.175333	184.763198	49.743617
720.080813	182.406901	49.748621
716.798453	174.618219	49.753626
713.428444	179.311914	49.758631
709.927937	181.303697	49.763636
705.742050	180.569382	49.768641
702.628348	168.248674	49.773645
699.237817	187.753559	49.778650
695.574843	168.564747	49.783655
692.354372	166.587778	49.788660
688.444945	177.021117	49.793665
685.231474	175.231425	49.798669
682.015321	180.002524	49.803674
678.205882	176.368547	49.808679
674.894099	171.812834	49.813684
670.932523	184.801967	49.818689
667.393170	179.361811	49.823693
664.103831	168.717766	49.828698
660.799674	169.382894	49.833703
657.146583	169.503167	49.838708
653.371931	168.872432	49.843713
650.182461	171.975817	49.848717
646.890382	181.220047	49.853722
643.203090	173.578294	49.858727
639.554371	178.543972	49.863732
636.054774	174.651380	49.868737
632.864489	168.073526	49.873741
629.076196	178.633786	49.878746
625.480586	178.194779	49.883751
622.463450	164.866595	49.888756
618.817314	185.829806	49.893761
615.116413	161.034168	49.898765
611.124955	173.367169	49.903770
608.058035	174.392003	49.908775
604.705611	173.898341	49.913780
600.948899	179.085893	49.918785
597.397841	169.300003	49.923789
593.799678	175.483729	49.928794
590.389045	164.449165	49.933799
587.280307	170.826714	49.938804
583.793569	182.407397	49.943809
580.351727	164.731231	49.948813
576.914635	164.025156	49.953818
573.067129	176.621290	49.958823
569.660365	165.634342	49.963828
565.759039	172.268789	49.968833
562.648465	166.853477	49.973837
558.972279	162.404781	49.978842
555.493088	178.964606	49.983847
552.307185	170.706872	49.988852
548.517929	174.460750	49.993857
545.582859	166.645394	49.998861
541.572325	168.583780	50.003866
537.700464	174.830794	50.008871
534.342167	161.707886	50.013876
530.762625	179.655100	50.018881
527.566648	178.205916	50.023885
524.124256	177.163641	50.028890
520.613414	171.042589	50.033895
517.146076	169.517776	50.038900
513.386083	185.096812	50.043905
510.225970	166.674600	50.048909
506.578501	168.821378	50.053914
502.672354	185.701348	50.058919
499.613102	169.976765	50.063924
496.041416	175.657072	50.068929
492.384828	177.640020	50.073933
488.841283	177.625879	50.078938
485.081913	164.804737	50.083943
482.010202	153.839165	50.088948
478.521637	174.579070	50.093953
475.226202	166.710022	50.098957
471.617285	169.594996	50.103962
467.995117	167.501885	50.108967
464.531783	158.293130	50.113972
460.860284	156.297455	50.118977
457.652159	167.344805	50.123981
454.211574	169.188900	50.128986
450.376070	160.806004	50.133991
447.187641	166.510136	50.138996
443.272033	175.214905	50.144001
439.632441	159.058828	50.149005
436.413743	170.049037	50.154010
432.885521	174.354055	50.159015
429.655115	166.886963	50.164020
425.830834	171.655237	50.169025
422.361655	167.930784	50.174029
419.214651	165.984044	50.179034
415.154725	168.959531	50.184039
412.070316	170.617548	50.189044
408.096925	179.121649	50.194049
404.588164	170.519262	50.199053
401.196421	169.668857	50.204058
397.768761	175.582711	50.209063
394.474149	164.145638	50.214068
390.911126	169.108825	50.219073
387.761261	157.298909	50.224077
384.239392	163.574605	50.229082
380.390272	184.099659	50.234087
376.873564	161.471223	50.239092
373.023359	173.470637	50.244097
369.633916	172.157081	50.249101
366.306952	168.892279	50.254106
362.785386	169.279848	50.259111
359.713919	167.163009	50.264116
356.012536	173.596726	50.269121
352.530173	156.721005	50.274125
349.017821	167.927666	50.279130
345.395787	173.199549	50.284135
341.619206	171.474547	50.289140
338.240096	173.700204	50.294145
334.965411	176.567427	50.299149
331.507894	170.270264	50.304154
327.203562	169.895233	50.309159
324.410822	158.918193	50.314164
320.795639	161.637654	50.319169
317.411488	170.357484	50.324173
313.809039	155.448180	50.329178
310.561717	165.290782	50.334183
307.180951	166.462310	50.339188
303.210372	168.106069	50.344193
299.539296	175.620795	50.349197
296.029683	170.691718	50.354202
292.587255	171.546205	50.359207
289.222249	174.837392	50.364212
285.855222	164.955699	50.369217
282.726897	169.863502	50.374221
279.117064	166.761202	50.379226
275.390325	170.508352	50.384231
271.472944	162.000989	50.389236
267.991404	167.931695	50.394241
264.718793	159.747355	50.399245
261.245429	163.424337	50.404250
257.879955	168.672028	50.409255
254.711346	169.092993	50.414260
250.716149	164.713074	50.419265
246.858139	157.088448	50.424269
243.355941	169.932913	50.429274
240.143053	161.315099	50.434279
236.877130	163.814714	50.439284
233.150812	168.148415	50.444289
229.979638	169.464216	50.449293
226.346418	165.690819	50.454298
222.879981	159.565478	50.459303
219.216965	165.464433	50.464308
215.737241	161.118251	50.469313
212.188966	165.332377	50.474317
208.531350	165.635468	50.479322
205.050681	169.131670	50.484327
202.141361	162.194610	50.489332
198.218998	174.010497	50.494337
194.841246	172.836870	50.499341
191.192943	164.231140	50.504346
187.495483	171.960314	50.509351
184.336251	167.661429	50.514356
180.435551	167.758459	50.519361
176.992264	163.496252	50.524365
173.705496	172.829469	50.529370
170.521939	173.762692	50.534375
166.744742	167.579912	50.539380
162.831042	167.013777	50.544385
159.783562	164.205752	50.549389
156.535490	155.096588	50.554394
152.445317	168.456533	50.559399
149.279879	162.859615	50.564404
145.463670	164.008467	50.569409
142.210538	158.176647	50.574413
138.788086	168.795858	50.579418
135.127412	172.583469	50.584423
131.891600	159.529281	50.589428
128.142654	160.158171	50.594433
124.500560	161.420328	50.599437
121.185877	156.010572	50.604442
117.600083	157.633481	50.609447
114.309187	164.065491	50.614452
110.526390	160.730045	50.619457
107.072614	156.891163	50.624461
103.445405	149.878830	50.629466
99.762126	156.265483	50.634471
96.697811	159.870123	50.639476
92.976950	165.826745	50.644481
89.772624	159.869294	50.649485
86.269606	159.129689	50.654490
82.312478	155.967991	50.659495
79.471503	160.935044	50.664500
75.691756	158.944856	50.669505
72.119138	162.045917	50.674509
68.815652	153.687251	50.679514
65.191169	161.851522	50.684519
61.482070	163.182795	50.689524
57.476009	158.100316	50.694529
54.351380	152.355242	50.699533
51.363818	153.977000	50.704538
47.538751	164.341362	50.709543
44.078578	151.976317	50.714548
40.346190	165.619523	50.719553
36.704253	160.363533	50.724557
33.888860	161.301984	50.729562
30.134235	157.163134	50.734567
26.612068	156.748042	50.739572
23.108838	159.094403	50.744577
19.761105	151.098037	50.749581
16.110435	157.182989	50.754586
12.471329	161.534359	50.759591
9.199579	162.331590	50.764596
5.311707	158.478773	50.769601
2.203892	151.894463	50.774605