Thu Jun 16 11:50:16 2022

Number of Points = 9931

Depth (nm)	Load (N)	Time (s)
-0.434643	74.012717	0.000000
-0.381408	81.129322	0.005005
-0.282121	75.545259	0.010010
-0.407942	84.572383	0.015014
-0.673343	56.483677	0.020019
-0.999700	49.130471	0.025024
-1.596624	46.772700	0.030029
-1.683256	36.232647	0.035034
-2.082750	29.224196	0.040038
-2.067404	26.123213	0.045043
-2.759963	22.230620	0.050048
-2.772008	22.580317	0.055053
-2.820869	9.008644	0.060058
-3.602748	23.909535	0.065062
-3.769913	2.059111	0.070067
-4.087968	2.599465	0.075072
-4.634685	3.002694	0.080077
-4.460142	-4.861021	0.085082
-4.760290	15.230198	0.090086
-5.230704	-0.216156	0.095091
-5.789071	-0.700950	0.100096
-5.929905	18.769857	0.105101
-5.898395	0.608590	0.110106
-6.198116	9.825705	0.115110
-5.907379	4.961273	0.120115
-5.985503	-0.881512	0.125120
-7.057543	6.371787	0.130125
-6.976611	7.010069	0.135130
-7.519361	9.409283	0.140134
-7.391171	0.473467	0.145139
-7.569581	14.531568	0.150144
-8.607402	5.763579	0.155149
-8.317079	-1.998026	0.160154
-9.035368	1.638793	0.165158
-9.560384	12.029131	0.170163
-9.088348	6.147910	0.175168
-9.051054	11.834477	0.180173
-8.895044	6.787011	0.185178
-10.319003	17.809703	0.190182
-10.606496	5.312637	0.195187
-10.840899	6.378701	0.200192
-10.746124	4.904112	0.205197
-10.600823	12.881903	0.210202
-10.941394	3.434790	0.215206
-10.771300	3.261813	0.220211
-11.613805	6.163084	0.225216
-11.903492	5.628562	0.230221
-12.045572	-2.101047	0.235226
-12.245924	3.325772	0.240230
-12.560594	-3.156555	0.245235
-12.902070	0.282543	0.250240
-13.736282	9.819722	0.255245
-13.791230	7.873946	0.260250
-13.584044	6.808737	0.265254
-14.031575	10.761194	0.270259
-14.043920	3.414621	0.275264
-14.291925	12.626349	0.280269
-14.234014	11.692353	0.285274
-15.026194	7.749736	0.290278
-15.263767	-1.400085	0.295283
-15.277269	15.387622	0.300288
-15.546385	13.427023	0.305293
-15.360930	4.039383	0.310298
-16.438326	13.102671	0.315302
-16.651294	17.511605	0.320307
-16.841998	4.491074	0.325312
-17.197879	13.464625	0.330317
-17.063288	8.886735	0.335322
-17.427799	17.507747	0.340326
-17.270107	1.906591	0.345331
-17.976896	11.836464	0.350336
-18.653649	26.136648	0.355341
-18.570085	-1.838944	0.360346
-18.506494	6.522690	0.365350
-18.588448	17.044517	0.370355
-18.916787	7.630699	0.375360
-19.508164	9.912561	0.380365
-19.703789	6.271892	0.385370
-20.290150	15.024765	0.390374
-20.456787	4.870866	0.395379
-20.300207	11.411291	0.400384
-20.622155	10.223888	0.405389
-20.432879	4.951619	0.410394
-21.325895	14.441892	0.415398
-21.378131	8.072459	0.420403
-21.376700	-1.284076	0.425408
-21.746936	9.952478	0.430413
-21.404316	12.117479	0.435418
-22.530697	10.735387	0.440422
-22.980870	8.816352	0.445427
-23.216072	6.001734	0.450432
-23.382790	7.804107	0.455437
-23.089041	6.004129	0.460442
-23.301397	5.661731	0.465446
-23.902323	10.924789	0.470451
-24.487097	0.989453	0.475456
-24.722445	6.392263	0.480461
-24.505382	-3.583142	0.485466
-24.854022	-2.681004	0.490470
-24.940535	0.685870	0.495475
-25.359170	4.380210	0.500480
-26.368131	7.996504	0.505485
-26.329989	3.440474	0.510490
-26.628308	10.267982	0.515494
-26.828069	5.234226	0.520499
-26.288352	5.111643	0.525504
-26.554763	15.063647	0.530509
-26.730365	7.313925	0.535514
-27.328494	8.356933	0.540518
-28.065343	2.834225	0.545523
-28.086801	4.501213	0.550528
-28.339984	8.481138	0.555533
-28.277370	7.448107	0.560538
-28.805346	14.419917	0.565542
-28.521480	9.037309	0.570547
-29.057020	6.690318	0.575552
-29.949062	16.692046	0.580557
-29.806575	-8.496748	0.585562
-29.827748	1.372200	0.590566
-29.933985	5.534518	0.595571
-29.925201	-2.813023	0.600576
-30.874582	10.633866	0.605581
-31.429183	9.366034	0.610586
-31.593942	7.892704	0.615590
-31.770629	8.507955	0.620595
-31.430919	0.985708	0.625600
-31.687561	19.484582	0.630605
-31.518384	-1.068288	0.635610
-32.767941	5.258994	0.640614
-33.080478	12.226868	0.645619
-33.092954	11.474188	0.650624
-33.394977	1.873913	0.655629
-33.227599	9.937531	0.660634
-33.323572	5.585877	0.665638
-33.596674	4.273301	0.670643
-34.440996	5.303624	0.675648
-34.875184	24.926992	0.680653
-34.887168	7.446909	0.685658
-34.939805	7.445104	0.690662
-35.045071	14.296744	0.695667
-34.830609	1.848336	0.700672
-35.912612	7.529474	0.705677
-35.952894	6.391020	0.710682
-36.469448	11.756349	0.715686
-36.368848	17.419136	0.720691
-36.229161	9.892552	0.725696
-37.096727	14.194698	0.730701
-37.477110	8.887237	0.735706
-37.810538	16.192110	0.740710
-38.139798	10.469551	0.745715
-38.102119	6.613245	0.750720
-38.123663	12.887049	0.755725
-37.894726	4.714930	0.760730
-38.314147	0.698779	0.765734
-39.027897	7.240282	0.770739
-39.240103	0.946320	0.775744
-39.852477	2.222630	0.780749
-39.844473	2.728732	0.785754
-39.991878	4.383485	0.790758
-39.934568	7.543295	0.795763
-39.779911	-0.931051	0.800768
-40.791367	2.757870	0.805773
-40.651331	1.411449	0.810778
-41.501509	4.334807	0.815782
-41.483141	6.720510	0.820787
-41.917820	6.974117	0.825792
-42.580027	0.975802	0.830797
-42.450603	-4.434354	0.835802
-42.924452	8.180830	0.840806
-42.890878	2.550929	0.845811
-43.067503	3.090207	0.850816
-43.168171	14.810698	0.855821
-43.075027	15.459885	0.860826
-43.122970	9.629376	0.865830
-43.854625	0.815635	0.870835
-44.290412	8.832530	0.875840
-44.526150	17.104139	0.880845
-44.507835	-0.569566	0.885850
-44.673952	7.065960	0.890854
-45.712812	9.487578	0.895859
-45.854703	3.114517	0.900864
-46.070048	8.623032	0.905869
-46.095869	4.756405	0.910874
-46.188942	15.520680	0.915878
-46.449809	5.612120	0.920883
-46.343565	7.508385	0.925888
-46.492744	10.582260	0.930893
-46.983172	4.541251	0.935898
-47.307452	12.717393	0.940902
-47.392064	6.186984	0.945907
-47.804782	6.755020	0.950912
-48.825932	12.739229	0.955917
-48.954575	7.714636	0.960922
-49.101188	3.065922	0.965926
-49.104977	7.375370	0.970931
-49.339275	1.968202	0.975936
-49.443303	12.072126	0.980941
-49.120358	7.203949	0.985946
-49.713919	18.386949	0.990950
-50.413331	1.359453	0.995955
-50.593600	4.874313	1.000960
-50.625903	15.306344	1.005965
-50.524182	6.151750	1.010970
-50.982958	6.191711	1.015974
-51.849014	8.000449	1.020979
-52.062573	3.780990	1.025984
-52.169981	3.026340	1.030989
-52.198677	-3.194459	1.035994
-52.289260	11.154549	1.040998
-52.568035	7.934863	1.046003
-53.178399	7.197926	1.051008
-53.986373	15.634541	1.056013
-53.576804	8.321631	1.061018
-53.727894	13.659415	1.066022
-54.224541	19.310511	1.071027
-53.785851	11.025000	1.076032
-54.090802	13.908963	1.081037
-54.378796	11.238127	1.086042
-55.017082	17.335457	1.091046
-55.753083	11.988213	1.096051
-55.739689	5.285736	1.101056
-55.880165	14.043251	1.106061
-55.766680	17.744657	1.111066
-55.787417	14.808966	1.116070
-56.731081	1.912290	1.121075
-56.865920	10.759631	1.126080
-57.513370	6.784323	1.131085
-57.280311	7.349517	1.136090
-57.590049	8.865657	1.141094
-57.569096	9.567222	1.146099
-57.615198	4.150557	1.151104
-58.419216	10.141402	1.156109
-58.437516	-4.476978	1.161114
-59.160013	-0.535116	1.166118
-59.225003	7.004380	1.171123
-58.717425	1.402493	1.176128
-59.174261	6.207665	1.181133
-59.616854	-4.492140	1.186138
-60.272083	5.251831	1.191142
-60.596382	1.669129	1.196147
-60.434587	8.561767	1.201152
-60.545463	9.872301	1.206157
-60.510043	8.471843	1.211162
-61.436258	-0.458607	1.216166
-61.977747	3.170208	1.221171
-62.140408	6.235162	1.226176
-62.202239	9.948177	1.231181
-62.365339	9.522564	1.236186
-62.705900	7.572199	1.241190
-62.745112	22.082211	1.246195
-62.425593	13.417539	1.251200
-63.256674	1.635979	1.256205
-63.677042	5.221496	1.261210
-64.000605	5.647635	1.266214
-64.052372	16.167920	1.271219
-63.733769	4.410730	1.276224
-64.450543	8.346223	1.281229
-64.985800	3.825174	1.286234
-65.587395	4.251684	1.291238
-65.518028	7.349421	1.296243
-65.624600	14.609698	1.301248
-65.723674	7.953234	1.306253
-65.664512	1.900619	1.311258
-65.767462	15.819277	1.316262
-66.060855	9.533108	1.321267
-66.821481	8.329812	1.326272
-67.145615	2.277701	1.331277
-66.936731	0.459291	1.336282
-67.778626	4.458376	1.341286
-68.235029	4.169629	1.346291
-68.722458	10.620557	1.351296
-69.084425	9.480514	1.356301
-68.266946	9.557965	1.361306
-68.804218	12.584303	1.366310
-68.956849	8.451553	1.371315
-68.695480	1.257352	1.376320
-69.209413	11.432173	1.381325
-70.009543	2.346028	1.386330
-70.905134	6.861951	1.391334
-70.504352	8.966530	1.396339
-70.502347	7.371821	1.401344
-70.743361	-5.391080	1.406349
-70.597648	-6.428472	1.411354
-70.929616	7.072348	1.416358
-71.246077	3.788652	1.421363
-71.773240	-2.095735	1.426368
-71.910122	11.463411	1.431373
-72.295355	0.520613	1.436378
-72.526364	11.912816	1.441382
-73.075413	10.110950	1.446387
-73.519465	14.781522	1.451392
-73.883274	16.767013	1.456397
-73.660242	3.089060	1.461402
-73.953617	15.012756	1.466406
-73.484427	12.536420	1.471411
-73.374069	12.647766	1.476416
-74.452571	14.673830	1.481421
-75.260942	5.647646	1.486426
-75.803774	13.614754	1.491430
-75.572442	15.801301	1.496435
-75.361077	14.361800	1.501440
-75.605908	16.341834	1.506445
-75.263715	10.358457	1.511450
-76.246283	15.023715	1.516454
-76.788811	7.834712	1.521459
-77.052828	2.451991	1.526464
-77.003378	3.118953	1.531469
-76.513127	5.152216	1.536474
-77.219011	8.008817	1.541478
-78.006520	17.252290	1.546483
-78.057855	5.710531	1.551488
-78.455983	18.800652	1.556493
-78.497048	1.606057	1.561498
-78.472413	10.468574	1.566502
-79.427508	11.249071	1.571507
-79.884135	4.316972	1.576512
-80.197632	7.115235	1.581517
-80.076802	-0.655548	1.586522
-80.334865	3.484507	1.591526
-80.442128	13.723724	1.596531
-80.144070	12.276308	1.601536
-80.425815	7.236277	1.606541
-80.823339	1.522443	1.611546
-81.676228	6.303001	1.616550
-81.751449	10.820080	1.621555
-81.517840	12.739491	1.626560
-82.071414	22.950467	1.631565
-81.938994	6.885383	1.636570
-82.490462	4.959024	1.641574
-82.762720	17.189987	1.646579
-83.262742	11.463790	1.651584
-83.912834	15.798958	1.656589
-83.808602	12.078844	1.661594
-83.644914	20.223868	1.666598
-83.515068	14.128689	1.671603
-83.991732	11.366312	1.676608
-84.809636	14.296872	1.681613
-84.723169	4.575475	1.686618
-85.165267	11.764531	1.691622
-85.216552	13.892522	1.696627
-85.148260	-0.888345	1.701632
-86.051417	10.099281	1.706637
-86.326199	9.864375	1.711642
-86.494919	-1.825786	1.716646
-86.882304	1.409982	1.721651
-86.525102	9.084111	1.726656
-87.028739	18.439895	1.731661
-87.231097	-1.083676	1.736666
-88.140552	6.360290	1.741670
-88.587160	10.808920	1.746675
-88.275296	8.235664	1.751680
-88.768446	9.060964	1.756685
-88.485755	0.834388	1.761690
-88.706487	-3.631204	1.766694
-88.446371	13.717588	1.771699
-88.646543	-1.446175	1.776704
-89.575289	9.353208	1.781709
-89.842177	13.783482	1.786714
-90.395048	4.434703	1.791718
-90.270488	2.825957	1.796723
-89.933236	0.131306	1.801728
-90.920789	14.075602	1.806733
-91.348917	-1.155553	1.811738
-91.562654	-1.512913	1.816742
-91.486533	9.549538	1.821747
-91.642999	5.187760	1.826752
-92.059362	4.090349	1.831757
-92.375161	5.937584	1.836762
-92.984006	3.114976	1.841766
-92.880475	8.119453	1.846771
-93.030655	7.656980	1.851776
-93.437591	0.910426	1.856781
-93.048766	3.472853	1.861786
-94.038128	6.125036	1.866790
-94.760371	9.910102	1.871795
-94.824446	-2.770464	1.876800
-95.046360	5.752193	1.881805
-94.613143	-0.470264	1.886810
-95.133826	2.472929	1.891814
-95.271457	-4.217405	1.896819
-95.231397	3.637580	1.901824
-95.369349	2.866177	1.906829
-95.871259	1.017358	1.911834
-96.442683	10.542087	1.916838
-96.657098	8.346341	1.921843
-96.192841	9.093321	1.926848
-97.454137	9.960336	1.931853
-97.628415	6.709177	1.936858
-98.096629	8.781276	1.941862
-98.131917	10.964433	1.946867
-98.430517	6.581554	1.951872
-98.432427	1.651840	1.956877
-98.175533	5.645526	1.961882
-98.198908	7.993338	1.966886
-98.738559	12.210219	1.971891
-99.087021	9.240794	1.976896
-99.598266	15.479907	1.981901
-99.514094	10.183377	1.986906
-100.676720	15.933885	1.991910
-101.156551	-0.170385	1.996915
-100.441905	12.390562	2.006912
-100.190627	10.196343	2.016909
-99.911262	4.803010	2.026906
-99.746001	1.751725	2.036902
-99.011091	4.311587	2.046899
-98.612627	8.849151	2.056896
-97.594755	0.248791	2.066893
-97.261134	6.087276	2.076890
-96.912205	9.211938	2.086886
-96.160943	7.812643	2.096883
-95.752032	8.051137	2.106880
-95.572646	2.803482	2.116877
-94.501649	5.891092	2.126874
-94.141373	-1.128677	2.136870
-93.985755	0.200418	2.146867
-93.575683	-3.231966	2.156864
-92.561901	5.608916	2.166861
-92.369922	5.924503	2.176858
-91.943212	7.366990	2.186854
-91.047147	3.551034	2.196851
-90.989465	12.159952	2.206848
-90.630176	9.205506	2.216845
-89.628917	9.849434	2.226842
-89.349992	12.508663	2.236838
-88.817721	18.175093	2.246835
-88.088500	16.946970	2.256832
-87.969622	9.312925	2.266829
-87.471056	11.976996	2.276826
-86.762834	8.655309	2.286822
-86.488849	10.166401	2.296819
-85.082994	10.292438	2.306816
-85.553528	5.163107	2.316813
-84.729990	6.010062	2.326810
-84.572156	5.594843	2.336806
-83.694730	15.037607	2.346803
-83.342240	7.369993	2.356800
-82.933331	12.778005	2.366797
-82.081249	13.275355	2.376794
-81.946929	12.010865	2.386790
-81.161448	7.823944	2.396787
-80.269595	7.916443	2.406784
-80.191055	11.168275	2.416781
-80.172629	8.860073	2.426778
-79.346203	10.811052	2.436774
-78.707907	11.245103	2.446771
-78.136124	12.777805	2.456768
-77.880368	8.009448	2.466765
-77.104931	12.670518	2.476762
-76.841460	10.934793	2.486758
-76.392972	11.121458	2.496755
-75.389858	11.321118	2.506752
-75.170314	6.702272	2.516749
-75.128467	10.510023	2.526746
-74.184201	5.800989	2.536742
-74.002022	3.715094	2.546739
-73.322667	6.453449	2.556736
-72.438100	12.207159	2.566733
-72.441306	5.874213	2.576730
-71.838292	8.762686	2.586726
-71.050750	10.164113	2.596723
-70.935612	15.894593	2.606720
-70.648556	13.961511	2.616717
-69.528005	9.092115	2.626714
-69.350756	12.243820	2.636710
-68.609983	12.198945	2.646707
-67.881762	10.696630	2.656704
-67.715023	9.613970	2.666701
-67.696798	12.732293	2.676698
-66.397895	15.768318	2.686694
-66.072159	15.404967	2.696691
-66.046688	15.546464	2.706688
-65.289514	8.597463	2.716685
-64.670207	8.279040	2.726682
-64.482403	16.249088	2.736678
-63.301131	14.488764	2.746675
-62.806069	12.011358	2.756672
-62.642793	7.861677	2.766669
-62.610634	8.430425	2.776666
-61.949303	2.703263	2.786662
-61.347465	14.791350	2.796659
-60.635782	8.949132	2.806656
-59.807953	13.077819	2.816653
-59.660067	4.087680	2.826650
-59.612179	8.669702	2.836646
-58.832723	11.528771	2.846643
-58.246207	16.124461	2.856640
-57.957987	4.138018	2.866637
-56.869010	10.428499	2.876634
-56.675644	8.702434	2.886630
-56.575248	15.021311	2.896627
-55.018092	11.275782	2.906624
-55.166771	14.120659	2.916621
-54.955929	9.284108	2.926618
-54.614021	13.256573	2.936614
-53.652765	14.982036	2.946611
-53.370930	15.241139	2.956608
-52.103220	13.535529	2.966605
-52.018570	12.030373	2.976602
-51.906243	4.436775	2.986598
-51.570404	7.693104	2.996595
-50.342884	12.491101	3.006592
-50.020324	10.585738	3.016589
-49.792600	3.864899	3.026586
-49.714433	5.461893	3.036582
-48.883155	10.207431	3.046579
-48.027530	7.515059	3.056576
-47.286691	5.912327	3.066573
-47.085381	7.850306	3.076570
-47.128045	4.649011	3.086566
-45.984050	3.540522	3.096563
-45.525713	8.451559	3.106560
-45.384234	-2.656582	3.116557
-44.712686	6.962551	3.126554
-44.115639	-4.644344	3.136550
-44.042693	10.630695	3.146547
-42.963515	7.577136	3.156544
-42.362520	12.723006	3.166541
-42.160640	-1.876646	3.176538
-42.127287	-1.510494	3.186534
-40.986910	3.873639	3.196531
-40.945430	5.531272	3.206528
-40.082348	4.404408	3.216525
-39.218453	10.533445	3.226522
-39.068745	2.489014	3.236518
-39.153457	5.698136	3.246515
-38.192741	4.853402	3.256512
-37.580850	-1.042106	3.266509
-37.224368	7.308319	3.276506
-36.206089	2.807436	3.286502
-35.937067	4.598798	3.296499
-35.875246	3.446452	3.306496
-35.363109	-2.057209	3.316493
-34.261679	4.149822	3.326490
-34.147976	-4.390010	3.336486
-34.013579	8.849058	3.346483
-33.105587	1.827525	3.356480
-32.534319	-4.108288	3.366477
-32.270919	-0.190118	3.376474
-31.457961	-0.367775	3.386470
-31.065200	8.091636	3.396467
-30.889631	2.325327	3.406464
-30.215172	-3.581015	3.416461
-29.441531	-8.192055	3.426458
-29.523997	-4.232780	3.436454
-28.564412	5.201452	3.446451
-27.836492	5.534364	3.456448
-27.501946	-4.543213	3.466445
-27.498961	3.268163	3.476442
-26.488828	1.272239	3.486438
-26.154894	2.369124	3.496435
-25.739789	-3.800918	3.506432
-24.762712	3.810563	3.516429
-24.660308	-5.367195	3.526426
-24.427293	1.232224	3.536422
-23.581988	1.078462	3.546419
-23.340198	2.546871	3.556416
-22.524580	4.805366	3.566413
-21.954482	2.136724	3.576410
-21.268026	-2.527376	3.586406
-21.495180	11.615466	3.596403
-20.875594	5.355917	3.606400
-19.867836	11.338993	3.616397
-19.763367	3.677595	3.626394
-18.961330	4.612470	3.636390
-18.458256	6.835246	3.646387
-18.081909	4.998092	3.656384
-18.041706	11.318670	3.666381
-17.126316	5.701989	3.676378
-16.647113	2.645249	3.686374
-15.902732	6.607064	3.696371
-15.211835	6.455755	3.706368
-15.118337	10.939564	3.716365
-14.874008	6.017517	3.726362
-13.944224	10.471139	3.736358
-13.718769	3.896916	3.746355
-13.475269	7.918886	3.756352
-12.413629	5.480267	3.766349
-11.625368	2.209072	3.776346
-11.569562	7.621313	3.786342
-11.401387	3.484949	3.796339
-10.266264	6.738991	3.806336
-9.942847	6.530913	3.816333
-10.134279	-0.017138	3.826330
-9.158212	5.579713	3.836326
-8.383593	8.754942	3.846323
-8.301907	2.648689	3.856320
-7.403008	3.047929	3.866317
-6.785533	-2.656968	3.876314
-6.580606	11.160510	3.886310
-6.319747	7.464152	3.896307
-5.238533	5.050106	3.906304
-4.959027	8.959938	3.916301
-4.994740	8.335239	3.926298
-4.053266	14.367156	3.936294
-3.823180	13.281733	3.946291
-3.458020	22.359730	3.956288
-3.017410	28.372778	3.966285
-2.244062	44.080883	3.976282
-2.053209	52.980216	3.986278
-1.392788	77.639617	3.996275
-0.993745	83.410384	4.006272
-0.787055	99.370632	4.016269
-0.583196	132.588204	4.026266
0.000000	142.112225	4.031270
0.572117	144.985836	4.036275
0.211677	176.639415	4.041280
0.366502	175.637897	4.046285
0.491421	189.890596	4.051290
0.698492	194.461216	4.056294
0.978039	205.608686	4.061299
1.081579	210.048438	4.066304
1.208018	214.965545	4.071309
1.106285	220.110072	4.076314
1.255452	216.809457	4.081318
1.407914	214.272869	4.086323
1.008643	212.512120	4.091328
0.806771	211.266183	4.096333
1.365885	223.133814	4.101338
1.327988	215.650680	4.106342
1.466383	219.720048	4.111347
0.821276	213.774555	4.116352
1.120233	211.180414	4.121357
0.923668	221.397538	4.126362
0.956188	217.216274	4.131366
1.109230	223.072024	4.136371
1.689189	239.489423	4.141376
1.468802	230.325177	4.146381
1.170808	222.996402	4.151386
1.070640	231.524720	4.156390
1.534033	241.021731	4.161395
1.581607	249.203240	4.166400
1.774987	242.544312	4.171405
1.117853	236.593892	4.176410
1.654024	240.219388	4.181414
1.676722	231.892798	4.186419
1.609756	233.440955	4.191424
1.259740	217.803317	4.196429
1.264058	235.727288	4.201434
1.475823	238.463257	4.206438
1.511988	235.791687	4.211443
1.796222	263.181608	4.216448
1.888473	253.552024	4.221453
1.774667	241.815199	4.226458
1.681331	225.123138	4.231462
1.935782	223.615630	4.236467
1.627354	226.660420	4.241472
1.706142	220.162106	4.246477
1.437301	222.381720	4.251482
1.461689	229.240740	4.256486
1.336371	213.363535	4.261491
0.984985	223.944137	4.266496
1.557884	241.783922	4.271501
1.557177	244.300671	4.276506
1.528389	262.504108	4.281510
1.792655	256.998276	4.286515
1.728570	249.385085	4.291520
1.822220	247.066471	4.296525
1.743838	261.755739	4.301530
1.468590	260.890694	4.306534
1.858888	250.041420	4.311539
1.787970	275.643041	4.316544
1.915212	253.284270	4.321549
2.143470	253.254988	4.326554
1.550931	248.872461	4.331558
1.879671	253.593862	4.336563
1.505018	254.500410	4.341568
2.131439	244.968522	4.346573
1.997902	259.609091	4.351578
1.702754	255.962412	4.356582
1.932307	253.649653	4.361587
1.532574	254.664426	4.366592
1.756275	246.670029	4.371597
1.675724	256.651853	4.376602
1.816104	268.744986	4.381606
1.701578	262.894995	4.386611
1.723997	273.857213	4.391616
2.022449	276.667455	4.396621
2.177975	290.753297	4.401626
1.870261	284.880272	4.406630
2.279497	283.388713	4.411635
1.995316	283.108884	4.416640
2.521121	272.706896	4.421645
2.325184	273.977939	4.426650
2.108501	266.072782	4.431654
2.169753	264.401565	4.436659
1.803091	263.591484	4.441664
1.714893	262.136354	4.446669
2.002601	267.315293	4.451674
2.130239	288.802679	4.456678
2.504752	289.242009	4.461683
2.166327	280.180504	4.466688
2.379610	285.254350	4.471693
2.568495	279.011781	4.476698
2.150696	264.871828	4.481702
2.174359	264.037593	4.486707
2.022238	266.386794	4.491712
2.130542	272.402872	4.496717
1.981308	287.167110	4.501722
2.395749	287.062173	4.506726
2.238113	278.742766	4.511731
1.892292	284.404549	4.516736
2.173811	283.613827	4.521741
2.166621	287.318966	4.526746
2.144692	281.701487	4.531750
2.333670	292.264660	4.536755
2.279846	293.244963	4.541760
2.092924	289.170185	4.546765
2.038637	302.843311	4.551770
2.239075	296.044189	4.556774
2.425738	279.419843	4.561779
2.172732	300.810130	4.566784
2.765028	305.894255	4.571789
2.621592	298.762764	4.576794
2.486119	291.235439	4.581798
2.849701	289.692330	4.586803
2.646220	292.480552	4.591808
2.853355	286.567136	4.596813
2.747075	287.726189	4.601818
2.680221	293.260385	4.606822
2.557747	290.659910	4.611827
2.437402	293.626969	4.616832
2.505129	284.542343	4.621837
2.558597	295.784459	4.626842
2.591334	296.549499	4.631846
2.068609	304.214213	4.636851
2.161055	305.321091	4.641856
2.270333	288.277907	4.646861
2.291779	298.317683	4.651866
2.395838	323.555141	4.656870
2.879430	325.474129	4.661875
2.882633	324.304097	4.666880
2.835890	324.467453	4.671885
2.838679	320.888332	4.676890
2.679466	335.261223	4.681894
2.869347	336.304548	4.686899
2.699621	339.269417	4.691904
2.747520	323.136469	4.696909
2.780058	320.046002	4.701914
2.552596	340.463923	4.706918
2.648127	323.945944	4.711923
2.793911	323.216127	4.716928
2.742546	329.423564	4.721933
2.650036	330.024521	4.726938
2.724811	328.487502	4.731942
3.067749	324.330678	4.736947
2.734112	336.630548	4.741952
2.787147	330.461610	4.746957
2.601427	325.684693	4.751962
2.654243	329.121548	4.756966
2.821414	324.604082	4.761971
2.853511	326.819360	4.766976
2.808778	319.780661	4.771981
2.847875	314.905822	4.776986
2.572937	330.036266	4.781990
2.909114	319.016236	4.786995
2.669084	326.341239	4.792000
2.954929	340.421277	4.797005
3.062241	360.890450	4.802010
3.178117	355.275920	4.807014
3.473586	357.014188	4.812019
3.343921	338.768266	4.817024
3.320168	324.401444	4.822029
3.267486	324.451342	4.827034
2.808279	333.397956	4.832038
3.229804	330.875290	4.837043
2.927500	333.271220	4.842048
3.092608	320.209575	4.847053
3.112664	322.921894	4.852058
2.628220	329.019571	4.857062
3.140847	331.232490	4.862067
3.159809	344.555654	4.867072
3.493770	346.166905	4.872077
3.054700	342.667604	4.877082
3.287978	339.351682	4.882086
3.583590	334.956827	4.887091
2.998677	336.280809	4.892096
3.031010	315.594940	4.897101
3.269697	338.135931	4.902106
3.541121	351.845151	4.907110
3.445413	328.512587	4.912115
3.253239	333.192535	4.917120
2.964200	333.396524	4.922125
3.024762	328.134267	4.927130
3.124974	343.694229	4.932134
3.434849	356.218859	4.937139
3.257957	364.924191	4.942144
3.335431	361.377409	4.947149
3.515761	358.026726	4.952154
3.493995	359.675946	4.957158
3.839845	352.068262	4.962163
3.526943	357.888892	4.967168
3.567950	363.551003	4.972173
3.281644	356.734720	4.977178
3.239981	351.438442	4.982182
3.535342	353.340101	4.987187
3.090552	367.621506	4.992192
3.434871	345.704910	4.997197
3.670733	357.019236	5.002202
3.103635	371.477225	5.007206
2.991097	362.135847	5.012211
3.053112	358.828196	5.017216
3.329086	360.048095	5.022221
3.114548	362.800471	5.027226
3.477996	390.399897	5.032230
3.748292	386.314452	5.037235
3.376245	386.302192	5.042240
3.694526	391.847856	5.047245
3.819536	393.337864	5.052250
3.532588	401.721141	5.057254
3.762126	392.082693	5.062259
3.682327	400.921661	5.067264
3.634796	395.563790	5.072269
3.745580	392.387867	5.077274
3.413730	394.143877	5.082278
3.803058	384.770851	5.087283
3.818155	400.112997	5.092288
3.538625	396.939322	5.097293
3.379267	397.462638	5.102298
3.613470	391.145844	5.107302
3.787050	388.111277	5.112307
3.570142	389.178717	5.117312
3.624316	391.676753	5.122317
3.646696	398.862534	5.127322
3.674318	403.381381	5.132326
3.897783	404.222047	5.137331
3.697380	405.861726	5.142336
4.000228	403.135896	5.147341
3.926764	403.176502	5.152346
3.426325	406.005333	5.157350
3.969709	415.659119	5.162355
4.028333	428.842322	5.167360
4.061123	420.574537	5.172365
3.891797	431.563917	5.177370
4.041981	431.364037	5.182374
4.117572	418.040669	5.187379
4.169149	417.439179	5.192384
4.377777	412.782933	5.197389
4.016443	404.692459	5.202394
3.512851	400.307718	5.207398
4.075136	414.738935	5.212403
4.178696	427.145985	5.217408
4.072874	407.625355	5.222413
4.051842	408.642472	5.227418
4.123225	417.201736	5.232422
4.158872	410.360539	5.237427
3.893895	406.878625	5.242432
4.322647	425.227337	5.247437
4.082837	421.344073	5.252442
4.205376	418.584404	5.257446
4.602370	424.777868	5.262451
4.131097	407.874786	5.267456
4.033041	401.688071	5.272461
3.962940	404.148341	5.277466
4.067004	430.819144	5.282470
4.057595	419.181444	5.287475
4.132911	418.105641	5.292480
4.176208	425.733802	5.297485
4.441281	427.483712	5.302490
4.248619	424.907243	5.307494
4.070861	432.205037	5.312499
3.992756	428.885305	5.317504
3.857462	425.563384	5.322509
4.149806	430.119589	5.327514
4.159976	433.102200	5.332518
3.762639	428.719623	5.337523
3.983965	440.636339	5.342528
4.573383	456.006853	5.347533
4.877137	461.183306	5.352538
4.815456	443.849938	5.357542
4.724594	437.156506	5.362547
4.503010	436.992511	5.367552
4.510714	423.886053	5.372557
4.295759	435.901992	5.377562
4.057859	420.492456	5.382566
4.321093	427.426634	5.387571
4.129120	440.594728	5.392576
4.549755	436.388927	5.397581
4.635163	459.830898	5.402586
4.489488	465.521135	5.407590
4.739997	447.611519	5.412595
4.531813	462.477417	5.417600
4.389428	457.587340	5.422605
4.411811	455.175798	5.427610
4.581407	462.334616	5.432614
4.940240	451.846745	5.437619
4.483923	459.126360	5.442624
4.270039	462.324471	5.447629
4.063852	456.259487	5.452634
4.549746	467.969031	5.457638
4.959177	464.591810	5.462643
4.491380	460.487732	5.467648
4.619273	455.210853	5.472653
4.623496	461.608343	5.477658
4.774842	459.648051	5.482662
4.892920	450.058373	5.487667
4.482892	460.267424	5.492672
4.189717	464.495585	5.497677
4.668051	456.802619	5.502682
4.380620	457.603902	5.507686
4.640393	465.785681	5.512691
4.597778	483.516142	5.517696
4.986471	489.338380	5.522701
4.902520	487.360931	5.527706
4.840712	482.850971	5.532710
5.034954	483.205657	5.537715
4.940685	497.500980	5.542720
4.985699	483.661999	5.547725
4.921365	475.944556	5.552730
4.893136	484.668106	5.557734
4.818608	467.293820	5.562739
4.705696	474.345130	5.567744
4.805501	485.246665	5.572749
4.934763	490.047868	5.577754
5.310471	491.243404	5.582758
5.259487	491.596883	5.587763
4.921178	491.623541	5.592768
5.241706	484.975067	5.597773
4.972977	471.027628	5.602778
5.045766	472.660840	5.607782
5.017252	465.988269	5.612787
4.873661	469.480501	5.617792
5.124202	478.382027	5.622797
5.275550	479.936554	5.627802
4.489992	486.127165	5.632806
5.271938	491.176855	5.637811
4.914941	496.975622	5.642816
5.135841	480.441196	5.647821
4.806862	490.313873	5.652826
4.615373	492.193894	5.657830
5.207578	479.044171	5.662835
5.026338	500.410446	5.667840
5.140759	488.368162	5.672845
4.833512	477.143876	5.677850
4.911508	492.311161	5.682854
4.899491	503.010987	5.687859
5.253545	513.034415	5.692864
5.418099	512.166624	5.697869
5.387939	519.179418	5.702874
5.490208	520.432969	5.707878
5.786356	495.087821	5.712883
5.526739	495.951794	5.717888
5.252094	498.000447	5.722893
5.205443	493.707983	5.727898
4.772370	482.074641	5.732902
5.041592	500.561682	5.737907
5.606922	504.631705	5.742912
5.726171	500.943519	5.747917
5.162456	496.516891	5.752922
5.251664	494.536872	5.757926
5.835809	500.797406	5.762931
5.101060	511.058277	5.767936
5.257950	514.927650	5.772941
5.628818	519.780686	5.777946
5.272384	509.536961	5.782950
5.963113	523.138764	5.787955
5.515919	516.110642	5.792960
5.417317	490.926531	5.797965
5.298333	505.577655	5.802970
5.406199	514.498242	5.807974
5.493414	514.899917	5.812979
5.586339	519.918553	5.817984
5.763249	537.422985	5.822989
5.673014	520.984327	5.827994
5.690481	527.939137	5.832998
5.559470	533.794297	5.838003
5.722879	523.950144	5.843008
5.643962	512.265751	5.848013
5.862561	520.484651	5.853018
5.592075	513.034086	5.858022
5.656853	505.222286	5.863027
5.632860	519.838291	5.868032
5.696616	526.844941	5.873037
6.025258	528.690117	5.878042
5.487852	511.737471	5.883046
5.783118	501.958854	5.888051
5.525670	522.398249	5.893056
5.870069	519.233319	5.898061
5.691347	519.036293	5.903066
5.853540	534.535891	5.908070
5.879654	521.356064	5.913075
5.721802	523.271571	5.918080
5.918855	521.607580	5.923085
5.861695	516.288254	5.928090
6.038394	521.641403	5.933094
5.888687	512.494608	5.938099
5.561055	504.976045	5.943104
5.562857	517.919212	5.948109
5.715869	523.987885	5.953114
5.599408	527.461933	5.958118
5.964628	522.967915	5.963123
5.507381	526.854429	5.968128
5.408851	520.426726	5.973133
5.760579	530.618759	5.978138
5.543003	534.452152	5.983142
6.111756	538.135971	5.988147
6.078315	556.513568	5.993152
5.889340	554.903993	5.998157
5.984484	544.889580	6.003162
5.885871	557.613289	6.008166
6.505701	552.495903	6.013171
5.945883	557.028606	6.018176
5.737144	552.908922	6.023181
6.123729	555.055195	6.028186
6.175254	555.493944	6.033190
6.480449	543.301703	6.038195
5.938548	546.268723	6.043200
5.872829	545.444805	6.048205
6.096876	549.565121	6.053210
6.076740	561.534362	6.058214
6.176441	551.651096	6.063219
6.100674	559.177849	6.068224
6.186566	561.103692	6.073229
6.176525	552.340850	6.078234
6.220298	565.643729	6.083238
6.194817	536.788284	6.088243
5.935804	541.212573	6.093248
6.282590	541.147623	6.098253
5.971980	525.102910	6.103258
5.886583	529.631987	6.108262
6.217013	542.998267	6.113267
6.346628	544.388577	6.118272
6.041282	527.881475	6.123277
5.874736	533.376491	6.128282
5.782189	546.342377	6.133286
6.176844	532.743120	6.138291
6.259289	558.758594	6.143296
6.191582	563.024699	6.148301
6.299717	553.153554	6.153306
6.013315	541.358895	6.158310
6.422914	531.178380	6.163315
5.819390	526.789892	6.168320
5.735601	517.212320	6.173325
5.925066	539.995064	6.178330
6.180125	557.882316	6.183334
6.351703	547.653123	6.188339
6.008773	555.637000	6.193344
6.102731	557.492647	6.198349
6.747587	552.829385	6.203354
6.023450	531.977986	6.208358
5.770476	532.687451	6.213363
5.710567	541.765908	6.218368
5.733694	537.747707	6.223373
6.136704	554.336653	6.228378
6.382011	560.300508	6.233382
6.577724	543.400511	6.238387
5.824340	544.159325	6.243392
6.182714	549.399985	6.248397
6.241319	549.183273	6.253402
6.237942	534.000846	6.258406
5.887116	513.819417	6.263411
5.862439	531.868293	6.268416
6.025761	548.216954	6.273421
6.431332	551.174400	6.278426
6.233603	541.722881	6.283430
6.386313	525.707756	6.288435
6.014279	533.982042	6.293440
5.975797	524.665323	6.298445
6.040355	516.548015	6.303450
5.927980	529.177687	6.308454
5.966564	526.361432	6.313459
6.121086	529.662545	6.318464
5.986274	552.626557	6.323469
6.206221	553.846852	6.328474
6.197010	540.629734	6.333478
6.402179	528.746156	6.338483
6.148434	530.783566	6.343488
6.095175	523.391907	6.348493
6.109229	526.246233	6.353498
5.780897	526.980977	6.358502
5.870419	518.930082	6.363507
5.901735	539.915693	6.368512
6.256027	552.299365	6.373517
6.542907	542.438644	6.378522
6.131713	544.334161	6.383526
5.982335	529.893493	6.388531
6.044299	524.107861	6.393536
5.897775	520.690500	6.398541
6.165629	525.905168	6.403546
6.012944	532.782338	6.408550
5.975554	532.362966	6.413555
6.077700	546.434187	6.418560
6.322315	549.288202	6.423565
5.839384	547.804158	6.428570
5.775148	558.641793	6.433574
6.511170	553.663648	6.438579
6.293442	564.440624	6.443584
6.066670	552.150416	6.448589
6.045065	530.052715	6.453594
6.048373	543.592427	6.458598
6.121423	543.712115	6.463603
6.014446	549.602080	6.468608
5.961277	553.585201	6.473613
6.168374	557.167584	6.478618
6.086599	558.448098	6.483622
6.159845	555.073731	6.488627
6.174814	547.428189	6.493632
5.764488	551.848284	6.498637
5.993689	558.710503	6.503642
5.830090	557.502607	6.508646
6.262686	563.158979	6.513651
6.384609	563.893804	6.518656
5.992535	556.166946	6.523661
6.491472	556.435371	6.528666
6.196956	547.501413	6.533670
6.098258	529.656019	6.538675
5.921268	538.505109	6.543680
6.054642	547.469151	6.548685
6.137509	542.947005	6.553690
6.197240	558.611940	6.558694
6.199397	548.314553	6.563699
5.853529	537.568578	6.568704
6.004972	542.816498	6.573709
6.363078	554.059565	6.578714
6.340101	546.191510	6.583718
6.012296	531.417171	6.588723
5.967567	536.522293	6.593728
5.913163	533.264130	6.598733
6.132444	531.015378	6.603738
5.870202	536.014774	6.608742
6.435434	542.636376	6.613747
6.139521	544.131832	6.618752
6.086150	527.957393	6.623757
6.337723	534.178189	6.628762
5.894777	537.340374	6.633766
6.210600	521.197078	6.638771
6.020075	531.367731	6.643776
6.250239	536.133036	6.648781
5.890163	530.765008	6.653786
5.942137	527.484926	6.658790
6.086835	526.325927	6.663795
5.995417	535.502619	6.668800
6.116013	550.237022	6.673805
6.175427	553.591248	6.678810
6.188267	553.329022	6.683814
6.455275	534.884326	6.688819
5.863493	532.530659	6.693824
5.546990	524.937044	6.698829
5.987700	539.721435	6.703834
5.869747	554.569354	6.708838
6.028650	545.637025	6.713843
6.061837	560.750123	6.718848
6.430503	560.948325	6.723853
5.879023	542.936426	6.728858
6.026111	556.702089	6.733862
5.993268	550.351915	6.738867
6.082721	559.993693	6.743872
6.298497	549.467144	6.748877
6.483436	547.450975	6.753882
6.162921	558.404658	6.758886
6.215472	545.936787	6.763891
6.213528	560.080765	6.768896
5.880717	538.183944	6.773901
6.039820	527.830348	6.778906
6.071210	551.740731	6.783910
6.195408	553.504661	6.788915
6.008772	556.823386	6.793920
6.241444	548.035828	6.798925
6.369795	552.779289	6.803930
5.973105	542.294369	6.808934
6.579796	530.384294	6.813939
6.170921	528.928364	6.818944
5.973489	521.585491	6.823949
5.799360	513.628285	6.828954
5.812808	519.958767	6.833958
6.161942	525.768615	6.838963
6.027995	535.909993	6.843968
6.156131	548.173974	6.848973
6.283354	534.323039	6.853978
6.098054	532.740187	6.858982
5.857289	517.828551	6.863987
6.173572	537.281302	6.868992
6.176155	530.495041	6.873997
6.150604	520.450866	6.879002
5.853294	526.623061	6.884006
6.112889	528.843590	6.889011
6.282782	532.678066	6.894016
6.092435	531.388466	6.899021
6.038968	523.192101	6.904026
5.844267	530.098411	6.909030
6.052978	540.187409	6.914035
6.087258	545.650229	6.919040
6.292710	554.763964	6.924045
6.514353	550.856007	6.929050
5.926518	525.573920	6.934054
5.956886	521.615300	6.939059
6.117847	533.227349	6.944064
6.033570	530.465433	6.949069
5.935813	544.129186	6.954074
5.894073	546.943506	6.959078
6.206092	545.196289	6.964083
5.846575	551.772511	6.969088
5.889828	557.070773	6.974093
6.230830	548.500807	6.979098
6.097505	550.825635	6.984102
6.232756	560.783734	6.989107
5.983839	545.913177	6.994112
6.021459	553.349663	6.999117
6.174463	553.196474	7.004122
5.965114	553.837861	7.009126
6.450491	548.430644	7.014131
6.094755	550.557226	7.019136
6.234481	552.774482	7.024141
6.332871	551.274086	7.029146
5.911745	549.194696	7.034150
6.191628	543.858139	7.039155
6.062515	547.634297	7.044160
6.332670	544.726891	7.049165
6.192234	523.931567	7.054170
5.600415	533.465315	7.059174
6.066186	537.300028	7.064179
6.210230	549.921477	7.069184
6.139460	546.519314	7.074189
6.122133	543.520113	7.079194
6.178516	547.788496	7.084198
6.338852	525.014436	7.089203
5.904910	527.964500	7.094208
5.709980	527.224188	7.099213
5.844056	543.437189	7.104218
5.894648	554.882611	7.109222
6.507244	543.778463	7.114227
6.196311	548.687845	7.119232
5.827567	549.098670	7.124237
6.149459	549.180097	7.129242
5.954492	554.570999	7.134246
6.184417	557.458618	7.139251
6.381730	549.165944	7.144256
6.066498	558.190018	7.149261
6.256880	545.529879	7.154266
6.211994	555.669378	7.159270
6.297420	537.677528	7.164275
6.112445	530.165764	7.169280
6.074288	531.548183	7.174285
6.018114	528.573556	7.179290
5.999971	525.530985	7.184294
5.849135	532.963878	7.189299
5.972647	546.158754	7.194304
6.281098	553.335809	7.199309
6.419964	559.255494	7.204314
6.023425	555.895127	7.209318
6.032474	528.440242	7.214323
6.091716	533.333138	7.219328
6.103423	532.708537	7.224333
6.350467	524.048548	7.229338
6.135005	534.911848	7.234342
6.019363	529.469588	7.239347
5.921979	528.179227	7.244352
6.041495	530.640541	7.249357
6.104240	526.549895	7.254362
5.847906	532.830058	7.259366
6.453996	537.020423	7.264371
6.286665	538.268015	7.269376
5.829768	533.469844	7.274381
6.237557	525.392199	7.279386
5.767859	534.873506	7.284390
6.093127	532.238066	7.289395
6.254571	549.353697	7.294400
5.882579	551.328667	7.299405
5.613584	547.695355	7.304410
5.768445	567.430044	7.309414
5.995983	561.783963	7.314419
6.309228	552.583726	7.319424
6.086830	555.729397	7.324429
6.361532	558.402143	7.329434
6.037250	569.948297	7.334438
6.667647	557.134931	7.339443
6.179827	549.945100	7.344448
6.021164	556.126951	7.349453
6.117468	548.353230	7.354458
6.100419	551.808094	7.359462
6.203837	558.357047	7.364467
6.095149	546.374870	7.369472
5.842265	539.913769	7.374477
5.868337	558.293175	7.379482
5.894193	565.968092	7.384486
6.248312	551.113798	7.389491
6.372622	560.222989	7.394496
6.302220	561.218086	7.399501
6.598086	554.048113	7.404506
6.006555	538.203220	7.409510
6.058961	534.429685	7.414515
5.477589	540.285277	7.419520
5.717964	542.688145	7.424525
6.222698	551.919644	7.429530
5.644870	566.474989	7.434534
6.384384	559.081446	7.439539
6.308544	559.682223	7.444544
6.225703	552.346444	7.449549
6.407180	556.534964	7.454554
6.228557	556.985996	7.459558
6.053865	536.932886	7.464563
6.139027	537.566940	7.469568
6.006247	548.658393	7.474573
6.401498	534.797695	7.479578
6.151852	539.737000	7.484582
6.068213	520.019885	7.489587
6.079831	525.285381	7.494592
5.973265	522.719135	7.499597
6.049997	522.057053	7.504602
5.896227	531.855716	7.509606
6.133929	540.547981	7.514611
6.216685	542.749394	7.519616
6.013183	544.124114	7.524621
6.127505	538.628063	7.529626
5.859891	531.941898	7.534630
6.134466	547.438131	7.539635
6.042047	554.612963	7.544640
6.168620	554.856696	7.549645
6.211161	549.881374	7.554650
6.076969	554.798350	7.559654
6.246788	548.833582	7.564659
6.046911	531.764463	7.569664
6.100343	527.715607	7.574669
6.062285	533.903268	7.579674
5.995236	538.451908	7.584678
6.173829	539.337684	7.589683
6.199733	543.900562	7.594688
6.127074	538.403347	7.599693
6.169861	524.582455	7.604698
6.069443	527.409724	7.609702
6.424524	533.002731	7.614707
6.364962	530.525005	7.619712
6.173153	526.972962	7.624717
6.304479	529.766375	7.629722
6.040924	536.116101	7.634726
6.268840	531.976454	7.639731
6.225876	536.165358	7.644736
6.102936	535.225306	7.649741
6.277607	526.545312	7.654746
6.000349	527.915151	7.659750
6.136415	532.640856	7.664755
6.205891	528.584316	7.669760
5.955608	520.899651	7.674765
6.415635	521.286382	7.679770
5.948965	526.660415	7.684774
6.159058	525.702621	7.689779
6.026421	524.267438	7.694784
6.086504	524.848020	7.699789
6.240894	528.830181	7.704794
6.083855	533.510697	7.709798
5.865369	528.650438	7.714803
5.960730	526.941097	7.719808
6.132477	537.719497	7.724813
6.240383	531.871812	7.729818
6.094341	534.918142	7.734822
5.911317	524.292066	7.739827
5.935127	519.237866	7.744832
6.019825	532.246370	7.749837
6.282985	529.545722	7.754842
6.278121	527.328684	7.759846
6.081069	525.484856	7.764851
6.268436	534.180600	7.769856
6.423772	525.217204	7.774861
6.355783	527.193925	7.779866
5.754293	533.474202	7.784870
5.860456	533.624920	7.789875
6.052249	530.497341	7.794880
5.733376	526.653555	7.799885
6.050850	517.279399	7.804890
5.651178	530.339532	7.809894
5.981741	531.671081	7.814899
6.002473	524.725651	7.819904
6.014697	526.514593	7.824909
6.088312	525.939350	7.829914
5.909249	531.214556	7.834918
6.142488	529.400842	7.839923
6.046745	534.578520	7.844928
6.019032	541.081162	7.849933
6.311148	524.563037	7.854938
6.092983	532.167767	7.859942
6.391168	526.279859	7.864947
6.456549	528.107669	7.869952
6.165981	533.017331	7.874957
6.650558	523.388154	7.879962
6.208479	520.598648	7.884966
6.708514	533.593765	7.889971
5.952833	528.401016	7.894976
6.036446	531.861537	7.899981
6.218036	528.365090	7.904986
6.199580	525.158210	7.909990
6.339187	528.516147	7.914995
6.176263	521.327987	7.920000
6.031600	512.054178	7.925005
6.053811	506.865284	7.930010
5.941898	515.758755	7.935014
6.212305	520.142806	7.940019
6.032109	524.736382	7.945024
6.059815	524.011270	7.950029
6.268543	527.361732	7.955034
6.096739	523.875344	7.960038
6.525738	507.803629	7.965043
6.196282	495.212664	7.970048
5.772679	503.441589	7.975053
6.137866	497.398878	7.980058
5.915189	496.010936	7.985062
5.808961	497.409928	7.990067
6.186557	496.866238	7.995072
5.985923	523.793352	8.000077
6.267296	528.350807	8.005082
6.243459	528.819767	8.010086
6.195677	511.529901	8.015091
6.312719	499.514108	8.020096
5.850468	498.353400	8.025101
6.034922	493.714938	8.030106
5.743698	498.222616	8.035123
6.039841	518.054513	8.040141
6.585092	521.973568	8.045158
5.861572	520.743859	8.050176
6.397946	513.552524	8.055194
6.172597	512.614725	8.060211
6.100494	487.116984	8.065229
6.095820	490.698257	8.070246
5.793738	504.599851	8.075264
5.863913	508.635393	8.080282
5.737527	510.686223	8.085299
6.042542	522.817680	8.090317
6.198530	531.426775	8.095334
6.145156	530.338140	8.100352
6.547601	528.326127	8.105370
6.320207	523.149783	8.110387
6.160936	522.240328	8.115405
6.309496	526.478231	8.120422
6.474417	526.337570	8.125440
6.429357	509.939140	8.130458
6.335666	505.350225	8.135475
6.068214	497.079585	8.140493
6.322490	493.596116	8.145510
6.087370	487.846871	8.150528
6.104144	486.520513	8.155546
5.986811	500.529241	8.160563
6.068858	511.295664	8.165581
6.173372	519.437472	8.170598
6.087071	518.004057	8.175616
6.317938	517.774364	8.180634
5.830714	527.059217	8.185651
6.422348	525.763128	8.190669
6.378679	522.885663	8.195686
6.274840	525.059120	8.200704
6.504419	514.662173	8.205722
6.351985	526.517235	8.210739
6.516273	529.728934	8.215757
6.518971	518.792235	8.220774
6.020850	507.270039	8.225792
6.586574	513.178598	8.230810
6.357964	512.238386	8.235827
5.940827	495.384440	8.240845
6.496244	506.702718	8.245862
6.215213	522.036573	8.250880
6.284121	516.352110	8.255898
6.287981	520.080571	8.260915
6.532183	526.118531	8.265933
6.390602	518.341440	8.270950
6.354437	524.506324	8.275968
6.483676	512.568016	8.280986
6.480702	501.453662	8.286003
6.087633	495.974755	8.291021
6.136010	511.190397	8.296038
6.024762	522.837806	8.301056
6.079266	518.564878	8.306074
5.984020	528.132620	8.311091
6.383127	529.741961	8.316109
6.292019	522.514187	8.321126
6.051664	529.800385	8.326144
6.602221	525.359968	8.331162
6.364369	526.461507	8.336179
6.240425	533.264590	8.341197
6.519916	530.486248	8.346214
6.327344	523.898930	8.351232
6.451253	521.313686	8.356250
6.434860	531.009314	8.361267
6.270066	528.582189	8.366285
6.558309	517.486712	8.371302
6.194617	527.776626	8.376320
6.681384	526.378797	8.381338
6.331764	531.135452	8.386355
6.078716	538.995779	8.391373
6.511578	518.325530	8.396390
6.586391	530.643824	8.401408
6.374874	526.448608	8.406426
6.589800	532.034909	8.411443
6.510220	522.489371	8.416461
6.488739	525.542438	8.421478
6.443936	525.659419	8.426496
6.463143	528.140920	8.431514
6.498530	528.115641	8.436531
6.420971	534.485065	8.441549
6.642341	528.073875	8.446566
6.609531	524.212340	8.451584
6.913216	525.444028	8.456602
6.709236	523.702667	8.461619
6.596848	528.783231	8.466637
6.719566	524.651950	8.471654
6.022719	538.026316	8.476672
6.610132	519.525248	8.481690
6.635424	532.402792	8.486707
6.338651	524.702514	8.491725
6.556621	515.628863	8.496742
6.201654	523.063893	8.501760
6.302444	540.197371	8.506778
6.763506	543.779530	8.511795
6.821565	554.054282	8.516813
7.015201	563.033080	8.521830
6.844544	546.842630	8.526848
6.485045	527.655195	8.531866
6.650244	527.413131	8.536883
6.391702	533.390798	8.541901
6.483618	516.446408	8.546918
6.759063	524.583983	8.551936
6.929840	524.343752	8.556954
6.634081	531.054091	8.561971
6.343895	526.769829	8.566989
6.732304	533.426938	8.572007
6.559989	537.609428	8.577024
6.611214	536.072789	8.582042
6.944523	552.220218	8.587059
6.629221	547.238474	8.592077
7.067072	536.712626	8.597095
6.586731	535.725054	8.602112
6.818624	518.314709	8.607130
6.580039	527.861363	8.612147
6.659413	536.778237	8.617165
6.590661	517.524956	8.622183
6.240768	536.569532	8.627200
6.533296	543.700073	8.632218
6.784271	556.061209	8.637235
6.954516	551.204695	8.642253
6.898575	553.684841	8.647271
6.628711	566.291472	8.652288
6.732793	555.473299	8.657306
6.868462	557.553944	8.662323
6.570001	572.664398	8.667341
6.439156	560.580685	8.672359
6.589226	562.689654	8.677376
6.695981	556.591919	8.682394
6.852641	564.344699	8.687411
6.398446	553.244551	8.692429
6.513600	551.324982	8.697447
6.292883	567.926014	8.702464
6.493017	552.866952	8.707482
6.990138	563.530280	8.712499
6.437170	583.598721	8.717517
6.969674	577.010236	8.722535
6.954564	591.460426	8.727552
6.805733	583.184799	8.732570
7.036264	568.953992	8.737587
6.885590	567.298778	8.742605
7.074898	559.232782	8.747623
6.972830	574.033674	8.752640
7.098519	561.733784	8.757658
7.183261	560.923344	8.762675
6.734470	560.131892	8.767693
6.987571	547.425900	8.772711
6.745714	565.756936	8.777728
6.567449	558.862872	8.782746
6.849163	553.674025	8.787763
6.489429	563.228913	8.792781
6.935349	568.543736	8.797799
6.762213	577.638358	8.802816
7.091179	584.101318	8.807834
7.427761	573.603398	8.812851
6.781245	571.631188	8.817869
6.618760	557.891335	8.822887
6.836118	566.967276	8.827904
6.666536	580.085781	8.832922
7.258414	596.764426	8.837939
7.188742	598.998572	8.842957
7.244983	584.280320	8.847975
7.069154	574.968131	8.852992
6.569730	570.362405	8.858010
6.629601	576.296720	8.863027
6.640206	585.752438	8.868045
6.936618	592.581042	8.873063
7.102036	596.473139	8.878080
6.949299	592.680706	8.883098
7.082140	597.292410	8.888115
6.959046	600.733468	8.893133
7.199958	592.780457	8.898151
6.901352	595.192564	8.903168
6.973974	598.393545	8.908186
7.281520	592.339076	8.913203
7.181824	593.977518	8.918221
7.157208	601.780840	8.923239
7.193454	598.379629	8.928256
7.465905	588.729725	8.933274
7.050438	597.887332	8.938291
7.033226	604.358010	8.943309
7.301854	591.728927	8.948327
6.971126	597.041521	8.953344
7.147892	591.714524	8.958362
7.531613	589.051400	8.963379
6.989986	587.468761	8.968397
6.943103	575.746380	8.973415
6.731033	572.228171	8.978432
6.769132	581.968555	8.983450
7.198050	585.934108	8.988467
6.742554	597.376606	8.993485
6.722466	590.344797	8.998503
6.758046	592.578474	9.003520
6.637355	584.246632	9.008538
7.124704	599.828412	9.013555
7.209555	613.364156	9.018573
7.387523	608.129948	9.023591
7.298665	602.754440	9.028608
7.230995	606.419855	9.033626
7.382824	599.645598	9.038643
7.127384	589.280139	9.043661
7.127455	588.861565	9.048679
7.100755	593.921988	9.053696
7.297369	595.678753	9.058714
7.338918	582.648218	9.063731
7.311885	592.837964	9.068749
7.384591	605.478647	9.073767
7.305577	597.468190	9.078784
7.298862	590.906614	9.083802
7.268471	594.701764	9.088819
7.189238	598.025752	9.093837
7.484845	589.491478	9.098855
7.344746	595.253377	9.103872
7.077419	591.098363	9.108890
7.323816	592.537613	9.113907
7.188870	599.741773	9.118925
7.331148	592.448730	9.123943
7.483233	584.168642	9.128960
7.268830	596.464619	9.133978
7.312590	594.438166	9.138995
7.182564	600.407021	9.144013
7.057409	585.123392	9.149031
7.544558	593.674943	9.154048
7.349274	611.129714	9.159066
7.387167	601.406873	9.164083
7.462438	604.102304	9.169101
7.568770	596.414100	9.174119
7.223796	601.941309	9.179136
7.227626	592.000526	9.184154
7.417899	592.839727	9.189171
7.359412	611.775819	9.194189
7.523522	607.284794	9.199207
7.766738	593.131381	9.204224
7.040211	600.596556	9.209242
7.359996	594.019992	9.214259
7.390206	602.156311	9.219277
7.529812	597.157533	9.224295
7.850814	604.686071	9.229312
7.229335	602.252430	9.234330
7.569252	593.559976	9.239347
7.439772	594.875061	9.244365
7.460760	594.657614	9.249383
7.503638	588.226989	9.254400
7.248664	591.347979	9.259418
7.447826	606.146849	9.264435
7.534561	616.190473	9.269453
7.514100	599.837577	9.274471
7.645236	603.206806	9.279488
7.372379	601.527693	9.284506
7.755063	615.587629	9.289523
7.554778	610.797347	9.294541
7.401422	592.951962	9.299559
7.981059	598.996121	9.304576
7.129082	595.761471	9.309594
7.492266	592.957675	9.314611
7.108539	609.202696	9.319629
7.610910	617.336179	9.324647
7.516429	607.085714	9.329664
7.773758	621.145214	9.334682
7.937023	608.525656	9.339699
7.329074	618.442791	9.344717
7.310758	616.700948	9.349735
7.568434	609.023743	9.354752
7.646939	611.922635	9.359770
8.055086	616.267537	9.364787
8.146387	616.521740	9.369805
7.720673	606.119460	9.374823
7.447257	600.184709	9.379840
7.152885	592.832158	9.384858
7.821442	597.308395	9.389875
7.697011	612.501720	9.394893
7.793596	618.624827	9.399911
7.892646	612.401302	9.404928
7.471606	607.036797	9.409946
7.648944	594.623643	9.414963
7.699386	600.492512	9.419981
7.629903	608.499472	9.424999
7.707666	604.230255	9.430016
7.762371	617.036094	9.435034
7.622934	608.240206	9.440051
7.607363	614.299087	9.445069
7.706990	611.029201	9.450087
7.971718	610.688618	9.455104
7.895523	610.208055	9.460122
7.670500	611.164399	9.465139
7.749881	609.067701	9.470157
7.625307	606.616597	9.475175
7.863977	616.096542	9.480192
7.635630	622.248548	9.485210
7.971408	613.609119	9.490227
7.530028	614.503796	9.495245
7.607118	614.283081	9.500263
7.998336	606.961095	9.505280
7.621271	620.126124	9.510298
7.736253	602.681373	9.515315
7.577003	607.478821	9.520333
8.008400	605.460440	9.525351
8.047172	604.771056	9.530368
7.614265	598.569709	9.535386
7.664742	616.027368	9.540403
7.754060	614.980291	9.545421
7.535195	600.866034	9.550439
7.741583	597.382977	9.555456
7.626525	618.308830	9.560474
7.468582	603.585706	9.565491
7.493128	610.258007	9.570509
7.953544	635.395590	9.575527
8.126581	631.253013	9.580544
7.805309	619.366438	9.585562
7.997963	606.552103	9.590579
7.896460	618.262134	9.595597
7.950704	613.107905	9.600615
7.983630	604.212488	9.605632
7.593783	611.229689	9.610650
8.153049	625.176218	9.615667
8.250735	642.868676	9.620685
8.185795	621.984449	9.625703
8.225491	613.835099	9.630720
7.628179	618.001246	9.635738
7.875830	611.002234	9.640755
7.728045	617.885952	9.645773
7.637329	632.070483	9.650791
8.329800	638.430393	9.655808
8.035735	646.556950	9.660826
8.351150	638.311640	9.665843
8.023744	624.714803	9.670861
7.667978	613.740836	9.675879
7.857253	627.256089	9.680896
8.236406	635.503626	9.685914
8.520475	631.216741	9.690931
8.244516	619.724762	9.695949
8.099500	614.437057	9.700967
8.040982	598.017140	9.705984
7.774854	607.830743	9.711002
8.027651	616.955473	9.716019
8.297701	627.052653	9.721037
7.941979	631.321075	9.726055
8.178897	632.930465	9.731072
8.329077	638.382749	9.736090
8.116142	620.226573	9.741107
7.659364	614.152074	9.746125
7.831318	635.890288	9.751143
7.830282	634.438639	9.756160
8.324799	636.774399	9.761178
8.234027	637.328321	9.766195
8.186188	637.259917	9.771213
8.058427	641.869139	9.776231
8.118253	639.420424	9.781248
8.148727	639.822348	9.786266
8.170436	641.384838	9.791283
8.502832	647.597900	9.796301
8.224591	646.739193	9.801319
8.378431	639.949726	9.806336
8.264259	642.468637	9.811354
8.254336	638.853240	9.816371
8.342233	629.116903	9.821389
8.427591	634.390271	9.826407
8.191867	641.671821	9.831424
8.367561	638.608212	9.836442
8.495977	633.341149	9.841459
8.586659	635.810363	9.846477
7.883475	631.026817	9.851495
8.160900	634.413209	9.856512
8.188178	634.235659	9.861530
8.492775	636.321463	9.866547
8.548606	646.783616	9.871565
8.381724	641.455824	9.876583
8.431435	635.674706	9.881600
7.912861	636.953522	9.886618
8.240268	634.938250	9.891635
8.324647	635.634945	9.896653
8.214452	647.916793	9.901671
8.487666	628.660100	9.906688
8.492880	630.336611	9.911706
8.203791	635.069519	9.916723
8.382871	632.935972	9.921741
8.382480	637.203835	9.926759
8.595922	636.908038	9.931776
8.210062	634.373460	9.936794
8.261904	641.788752	9.941811
8.442218	639.538291	9.946829
8.306872	643.521334	9.951847
8.439367	633.669476	9.956864
8.135169	635.939038	9.961882
8.458780	642.385392	9.966899
8.733623	634.058421	9.971917
8.407674	638.982620	9.976935
8.490899	633.933809	9.981952
8.314119	645.356656	9.986970
8.173369	640.782957	9.991987
8.795619	644.142086	9.997005
8.698539	646.758448	10.002023
8.653578	633.559230	10.007040
8.491682	650.816736	10.012058
8.435293	645.842459	10.017075
8.474036	633.555207	10.022093
8.252897	638.832779	10.027111
8.643015	638.441265	10.032128
8.738901	646.581318	10.037146
8.472550	639.828126	10.042163
8.547682	646.241838	10.047181
8.329958	652.245772	10.052199
8.425925	648.461133	10.057216
8.668710	644.053927	10.062234
8.485225	643.310441	10.067251
8.782067	639.126738	10.072269
8.389933	649.126019	10.077287
8.210867	643.283217	10.082304
8.518417	642.328986	10.087322
8.275496	668.011604	10.092339
8.585025	666.930692	10.097357
8.505934	674.504518	10.102375
8.839770	662.270230	10.107392
9.062114	662.043026	10.112410
8.554174	665.386901	10.117427
8.986020	665.083943	10.122445
8.920203	656.213768	10.127463
8.926073	644.298501	10.132480
9.164343	645.615207	10.137498
8.792017	643.782777	10.142515
8.613750	632.740004	10.147533
8.723393	646.508345	10.152551
8.765370	640.963890	10.157568
8.351904	642.619943	10.162586
8.566591	635.174982	10.167603
8.947401	630.707479	10.172621
8.643638	632.157842	10.177639
8.865879	626.503894	10.182656
8.503437	637.603846	10.187674
8.493507	639.421514	10.192691
8.674917	636.469144	10.197709
8.863834	664.402270	10.202727
8.995925	653.885933	10.207744
9.124606	660.338036	10.212762
8.877322	649.412343	10.217779
8.664637	644.431421	10.222797
8.439141	643.232175	10.227815
8.642819	655.976920	10.232832
9.007757	668.541120	10.237850
8.638338	671.075746	10.242867
9.150922	663.581936	10.247885
8.818525	665.837760	10.252903
8.846637	669.339951	10.257920
9.226476	663.953392	10.262938
8.962239	670.579463	10.267955
9.395300	658.230080	10.272973
8.871710	647.171345	10.277991
8.664568	640.170620	10.283008
9.124770	647.775664	10.288026
8.833172	657.745053	10.293043
9.064079	645.660339	10.298061
8.913750	651.930147	10.303079
8.848837	659.392393	10.308096
9.003161	659.683416	10.313114
9.021625	673.019497	10.318131
9.126944	656.022651	10.323149
9.117021	668.992824	10.328167
9.025028	655.767606	10.333184
9.041608	644.689869	10.338202
8.694668	650.639875	10.343219
9.374725	656.838393	10.348237
8.997076	650.629862	10.353255
9.059070	659.728187	10.358272
9.136393	658.358449	10.363290
9.028022	659.902387	10.368307
9.147657	642.106104	10.373325
8.946042	641.241918	10.378343
9.098297	652.323840	10.383360
9.205115	655.860158	10.388378
8.827662	663.071161	10.393395
9.104595	660.667751	10.398413
9.406997	662.254316	10.403431
9.239204	678.399467	10.408448
9.666568	661.446325	10.413466
9.094641	648.671117	10.418483
8.994955	636.259032	10.423501
9.005869	633.764278	10.428519
8.885245	634.257595	10.433536
9.057962	651.174234	10.438554
9.133431	663.298371	10.443571
9.193660	659.761812	10.448589
9.303432	674.930076	10.453607
9.304155	664.752110	10.458624
9.289888	665.964713	10.463642
9.087508	662.432482	10.468659
9.271339	670.006353	10.473677
9.334300	670.940598	10.478695
9.115731	669.133632	10.483712
9.271731	666.407458	10.488730
9.039277	668.254818	10.493747
9.389128	659.824904	10.498765
9.475453	668.735786	10.503783
9.400319	661.384169	10.508800
9.394200	657.108822	10.513818
9.094896	665.833970	10.518835
9.344688	654.319144	10.523853
9.634910	664.155980	10.528871
9.243705	657.116289	10.533888
9.335282	651.691560	10.538906
9.128846	672.325464	10.543923
9.306921	658.479940	10.548941
9.382845	662.258916	10.553959
9.285720	675.628173	10.558976
9.419051	663.393953	10.563994
9.232979	672.149990	10.569011
9.312475	664.937451	10.574029
9.243219	666.538888	10.579047
9.025126	669.911130	10.584064
8.998044	663.907797	10.589082
9.031441	670.406649	10.594099
9.261540	660.183499	10.599117
9.222772	668.856147	10.604135
9.217706	684.673391	10.609152
9.662295	696.959741	10.614170
9.583917	702.495578	10.619187
9.557653	704.024475	10.624205
9.270774	693.127238	10.629223
9.530869	696.303164	10.634240
10.024278	690.915246	10.639258
9.250385	684.177416	10.644275
9.489100	677.963259	10.649293
9.886538	676.531960	10.654311
9.348896	684.369031	10.659328
9.503033	673.462598	10.664346
9.352456	683.298288	10.669363
9.750100	693.675351	10.674381
9.790042	698.071775	10.679399
9.356381	681.522362	10.684416
9.533058	684.147025	10.689434
9.474004	691.980194	10.694451
9.803655	699.486881	10.699469
9.787181	693.516423	10.704487
9.390090	696.193097	10.709504
9.751523	695.572510	10.714522
9.529532	700.702536	10.719539
10.128547	700.680849	10.724557
9.793500	678.242874	10.729575
9.103629	675.606885	10.734592
9.832398	684.868114	10.739610
10.001862	692.201997	10.744627
10.119122	685.660535	10.749645
9.992689	669.597069	10.754663
9.415800	672.791544	10.759680
9.664090	669.133864	10.764698
9.517218	664.424385	10.769715
9.566047	661.575793	10.774733
9.697377	683.470561	10.779751
9.752712	698.193308	10.784768
10.075428	687.024015	10.789786
9.849926	677.539299	10.794803
9.281218	661.160719	10.799821
9.708584	677.377071	10.804839
9.914600	698.381641	10.809856
9.990635	695.295915	10.814874
10.216191	696.901383	10.819891
9.620116	686.265737	10.824909
9.904750	694.681159	10.829927
9.888979	681.905633	10.834944
10.420419	681.570570	10.839962
9.840338	672.374525	10.844979
9.608115	672.595890	10.849997
9.688568	670.629099	10.855015
9.665495	682.791775	10.860032
10.152026	672.197862	10.865050
9.420305	674.121920	10.870067
9.885145	693.362204	10.875085
10.168422	686.611059	10.880103
9.914735	687.776632	10.885120
10.431251	684.377909	10.890138
9.955131	677.619413	10.895155
10.052341	663.819229	10.900173
10.165529	661.214774	10.905191
10.026332	666.724238	10.910208
9.785861	657.433702	10.915226
9.802659	664.524251	10.920243
9.634882	660.870086	10.925261
9.958447	672.014639	10.930279
9.900186	694.913199	10.935296
9.836578	689.075016	10.940314
10.086333	683.995224	10.945331
9.805319	696.106461	10.950349
9.932505	689.036886	10.955367
9.520514	701.051979	10.960384
10.011043	686.791285	10.965402
9.723932	688.364467	10.970419
9.752127	693.336930	10.975437
10.237156	684.699268	10.980455
9.875274	703.557781	10.985472
9.830809	696.781674	10.990490
10.308617	708.016883	10.995507
10.334849	724.733937	11.000525
10.024080	713.193812	11.005543
10.333316	709.849707	11.010560
10.617479	704.628521	11.015578
10.347253	707.250185	11.020595
10.212341	697.494533	11.025613
10.358954	689.856504	11.030631
9.993099	703.570331	11.035648
10.096316	695.022525	11.040666
9.918769	690.543162	11.045683
9.904166	689.872532	11.050701
10.193013	711.360776	11.055719
10.115283	714.639471	11.060736
10.576324	705.829812	11.065754
10.302524	712.430617	11.070771
10.574851	715.253708	11.075789
10.857287	701.326641	11.080807
10.231836	698.675869	11.085824
10.399687	688.681054	11.090842
10.529909	690.886018	11.095859
10.119852	693.110987	11.100877
10.136267	688.182725	11.105895
9.895090	692.082206	11.110912
10.036243	699.253579	11.115930
10.542538	712.618212	11.120947
10.344849	721.273854	11.125965
10.494314	712.503182	11.130983
10.396370	727.430090	11.136000
10.620537	716.629846	11.141018
10.309336	700.799598	11.146035
10.071350	713.895964	11.151053
10.459163	713.176842	11.156071
10.426578	723.963538	11.161088
10.484324	721.956506	11.166106
10.375323	716.957934	11.171123
10.398873	717.804519	11.176141
10.756450	718.723145	11.181159
10.255153	721.404448	11.186176
10.243015	706.472226	11.191194
10.488778	717.171885	11.196211
10.319983	728.773951	11.201229
10.610656	715.442441	11.206247
10.451096	715.923300	11.211264
10.246955	719.681655	11.216282
10.822859	713.057796	11.221299
10.475108	724.060224	11.226317
10.612868	720.904757	11.231335
10.230576	716.464633	11.236352
10.954994	714.145306	11.241370
10.879037	720.636467	11.246387
10.087999	720.891528	11.251405
10.468918	709.567254	11.256423
10.616400	728.041781	11.261440
10.379733	723.670780	11.266458
9.944876	720.893644	11.271475
9.882694	727.884009	11.276493
10.450306	734.140897	11.281511
10.432083	747.565865	11.286528
10.574640	750.379508	11.291546
11.165755	738.891172	11.296563
11.008895	745.644287	11.301581
11.110344	747.431360	11.306599
11.031196	740.098573	11.311616
10.799447	729.870711	11.316634
10.765573	719.646861	11.321651
10.482901	717.999863	11.326669
10.923142	724.282026	11.331687
11.139093	731.032275	11.336704
11.118765	717.986068	11.341722
10.988074	713.955066	11.346739
10.760382	706.989197	11.351757
11.227415	705.528977	11.356775
10.763102	720.107545	11.361792
10.642820	722.154736	11.366810
10.983656	708.889829	11.371827
10.735680	719.101705	11.376845
11.251867	703.925909	11.381863
10.749055	709.058948	11.386880
10.797764	707.029990	11.391898
11.227868	705.068098	11.396915
11.158023	704.532950	11.401933
10.970267	705.312998	11.406951
10.875343	707.052021	11.411968
11.009519	715.865867	11.416986
10.777388	707.173904	11.422003
10.662152	710.186803	11.427021
10.967211	710.144612	11.432039
11.003412	709.524925	11.437056
10.869469	708.507553	11.442074
11.151452	704.197376	11.447091
10.673829	707.526506	11.452109
10.715234	701.892181	11.457127
10.743412	710.079473	11.462144
10.899448	701.400321	11.467162
10.909811	704.365402	11.472179
10.818100	724.042018	11.477197
10.980854	725.437831	11.482215
11.168414	730.075173	11.487232
11.224920	740.792150	11.492250
11.175323	738.919563	11.497267
10.897975	730.960213	11.502285
11.257025	740.015205	11.507303
11.253243	738.418457	11.512320
11.051331	721.416315	11.517338
11.108224	725.166568	11.522355
10.894564	741.433220	11.527373
11.186961	731.870464	11.532391
11.410433	737.114648	11.537408
10.943488	738.297063	11.542426
11.460534	733.304655	11.547443
11.331408	732.483985	11.552461
11.559668	729.676286	11.557479
11.369983	717.111915	11.562496
11.148891	710.032968	11.567514
11.229316	704.602191	11.572531
11.215312	717.376760	11.577549
11.466056	708.091814	11.582567
11.010996	703.387001	11.587584
10.813540	712.644154	11.592602
11.587495	726.970867	11.597619
11.444127	727.157474	11.602637
11.157617	721.916043	11.607655
11.318638	716.208904	11.612672
11.300861	734.062941	11.617690
11.393404	731.640886	11.622707
11.411959	736.069590	11.627725
11.333011	716.473126	11.632743
11.339257	724.401012	11.637760
11.314703	742.156690	11.642778
11.451008	743.917534	11.647795
11.445971	739.278178	11.652813
11.166710	730.229789	11.657831
10.941729	736.537848	11.662848
11.189412	739.864723	11.667866
11.331146	727.977027	11.672883
10.879318	739.107962	11.677901
11.072656	742.485738	11.682919
11.827965	744.239449	11.687936
11.481959	746.215896	11.692954
11.706680	737.288018	11.697971
11.411215	739.394175	11.702989
11.597531	750.062940	11.708007
11.502281	728.853720	11.713024
11.270872	739.479030	11.718042
11.450378	736.066513	11.723059
11.051137	733.701420	11.728077
11.369851	753.795392	11.733095
11.996794	761.863985	11.738112
11.904153	760.623094	11.743130
11.682571	740.250915	11.748147
11.461205	741.081588	11.753165
11.772484	740.707134	11.758183
12.043418	735.597749	11.763200
11.913711	750.807631	11.768218
11.914141	741.392999	11.773235
11.622521	735.280726	11.778253
11.728602	736.269747	11.783271
11.720488	732.624409	11.788288
11.894164	745.540493	11.793306
11.871471	745.643588	11.798323
11.935205	733.129433	11.803341
11.731637	728.841920	11.808359
11.980811	732.143748	11.813376
11.201510	741.559656	11.818394
11.812012	733.870336	11.823411
11.909054	745.683750	11.828429
11.788073	743.844510	11.833447
12.306108	738.153056	11.838464
12.006387	736.819344	11.843482
11.938479	736.696590	11.848499
11.611681	738.912530	11.853517
11.666395	731.133300	11.858535
11.694760	737.123662	11.863552
11.550893	747.156375	11.868570
11.842319	724.872925	11.873587
11.923591	736.021056	11.878605
11.208914	748.310276	11.883623
11.763396	736.991546	11.888640
11.598448	741.327174	11.893658
11.726490	736.790901	11.898675
12.067729	737.590106	11.903693
11.864356	736.513648	11.908711
11.971482	736.079052	11.913728
11.696543	755.246524	11.918746
12.254525	761.430915	11.923763
12.112354	745.290164	11.928781
11.521534	735.293747	11.933799
12.218683	755.799600	11.938816
11.983938	760.793395	11.943834
12.328488	765.188311	11.948851
12.027125	752.786137	11.953869
11.897656	744.033200	11.958887
11.936293	752.320047	11.963904
12.070723	758.677657	11.968922
12.167538	759.991081	11.973939
12.189367	769.982749	11.978957
12.296571	757.947813	11.983975
12.239971	741.809064	11.988992
11.779474	747.570924	11.994010
12.331238	749.143845	11.999027
12.322125	762.162576	12.004045
11.874760	758.234475	12.009063
12.445786	755.342181	12.014080
12.104467	757.869027	12.019098
12.188165	760.556106	12.024115
12.602462	764.530519	12.029133
12.173549	749.229220	12.034151
11.950263	730.799874	12.039168
11.769576	751.009926	12.044186
11.907743	741.179302	12.049203
12.470607	756.873247	12.054221
12.269463	771.237049	12.059239
12.403979	763.110919	12.064256
11.944886	762.600042	12.069274
12.368354	755.867031	12.074291
12.340068	753.919970	12.079309
12.261887	767.128627	12.084327
12.283456	762.205886	12.089344
12.415987	766.018339	12.094362
12.472036	768.816661	12.099379
12.354514	765.085085	12.104397
12.118223	767.157160	12.109415
12.388167	754.618851	12.114432
12.531184	762.478395	12.119450
12.359928	766.643551	12.124467
12.252694	762.154712	12.129485
12.447525	766.302965	12.134503
12.287644	766.628889	12.139520
12.278279	758.978518	12.144538
12.509142	760.522104	12.149555
12.835249	761.923696	12.154573
12.174448	770.241703	12.159591
12.595843	756.125218	12.164608
12.468981	768.139496	12.169626
12.533714	762.883405	12.174643
12.498326	763.882225	12.179661
12.249069	761.360674	12.184679
12.268898	757.159342	12.189696
12.426008	770.457246	12.194714
12.788445	783.315993	12.199731
12.820131	791.929734	12.204749
12.725545	772.743088	12.209767
12.950580	761.268782	12.214784
12.848892	756.031928	12.219802
12.211363	759.868898	12.224819
12.258657	756.794798	12.229837
12.528734	767.179609	12.234855
12.956934	791.871187	12.239872
13.073781	789.785593	12.244890
12.578266	768.227187	12.249907
12.639408	762.031712	12.254925
12.622114	778.674341	12.259943
13.008480	771.703898	12.264960
12.822036	775.595733	12.269978
12.844055	765.525872	12.274995
12.856395	761.190173	12.280013
12.720995	763.654060	12.285031
13.001435	757.860354	12.290048
13.150010	761.763739	12.295066
12.972102	755.752920	12.300083
13.042482	751.349770	12.305101
12.724661	760.214717	12.310119
12.894736	757.218930	12.315136
12.680592	762.096351	12.320154
12.680349	760.558059	12.325171
12.647401	757.542289	12.330189
12.405221	759.925711	12.335207
12.842756	764.891171	12.340224
13.104931	783.900445	12.345242
13.349297	781.254119	12.350259
13.283772	769.066946	12.355277
12.823401	762.195987	12.360295
12.974885	761.692556	12.365312
12.852946	759.069962	12.370330
12.932924	768.671582	12.375347
13.182121	770.664414	12.380365
13.101038	769.771052	12.385383
13.342661	759.000269	12.390400
12.982434	755.567021	12.395418
12.611732	749.984640	12.400435
12.744766	765.315653	12.405453
12.839058	782.891041	12.410471
13.180756	781.722537	12.415488
13.075076	792.900029	12.420506
13.238243	785.060338	12.425523
13.463486	778.855255	12.430541
13.582683	794.737790	12.435559
13.063041	779.271960	12.440576
12.924394	774.058035	12.445594
13.128881	780.162097	12.450611
13.580839	785.445592	12.455629
13.480554	789.883223	12.460647
13.315631	786.365341	12.465664
13.175830	758.497786	12.470682
12.971514	755.819922	12.475699
13.344585	770.907868	12.480717
13.393262	783.440191	12.485735
13.163418	766.492999	12.490752
13.034626	767.397433	12.495770
13.217929	786.939822	12.500787
13.328931	786.055752	12.505805
13.351748	790.883495	12.510823
13.370519	782.703956	12.515840
13.333970	779.243488	12.520858
13.247536	778.164432	12.525875
13.333720	773.577596	12.530893
13.453521	794.765706	12.535911
13.611896	780.951276	12.540928
13.303541	785.838663	12.545946
13.234098	790.912415	12.550963
13.452936	790.901890	12.555981
13.078471	786.393732	12.560999
13.097106	785.278615	12.566016
13.424616	787.905136	12.571034
13.524260	786.369132	12.576051
13.480084	793.188374	12.581069
13.324946	784.890357	12.586087
13.280600	783.355022	12.591104
13.199877	782.076044	12.596122
13.161705	792.396183	12.601139
13.604148	794.074953	12.606157
13.289499	813.601355	12.611175
13.739089	815.138422	12.616192
13.641497	806.246546	12.621210
13.464500	816.236363	12.626227
14.174360	810.001174	12.631245
13.891659	798.661720	12.636263
14.094086	796.087860	12.641280
13.794147	784.712788	12.646298
13.675150	793.740728	12.651315
13.828059	781.191624	12.656333
13.622781	777.576889	12.661351
13.765729	783.310092	12.666368
13.633355	779.911710	12.671386
13.346443	782.450727	12.676403
13.552261	772.026731	12.681421
13.621428	789.716396	12.686439
13.591016	809.169449	12.691456
13.712131	812.897498	12.696474
13.437886	817.294311	12.701491
14.112888	807.578240	12.706509
13.789232	813.319676	12.711527
14.013818	809.864760	12.716544
13.933153	805.146658	12.721562
13.484715	809.856060	12.726579
13.967332	810.629938	12.731597
13.989119	814.627405	12.736615
14.070446	818.675750	12.741632
13.862339	810.257462	12.746650
13.890784	805.123276	12.751667
14.186533	812.656384	12.756685
14.081968	815.445929	12.761703
13.807854	811.509258	12.766720
14.002906	811.020275	12.771738
13.568503	808.336337	12.776755
13.774564	801.373142	12.781773
13.876164	815.212439	12.786791
13.908570	814.123582	12.791808
13.845079	802.363229	12.796826
13.566158	810.017872	12.801843
13.642663	810.368796	12.806861
13.989321	826.246840	12.811879
14.111267	830.470725	12.816896
14.512763	831.679486	12.821914
14.436995	825.921493	12.826931
14.639965	805.460766	12.831949
14.531939	805.838346	12.836967
14.223544	802.331278	12.841984
14.363620	799.817121	12.847002
14.279006	790.239578	12.852019
14.549278	794.592260	12.857037
14.174027	808.337157	12.862055
14.339851	799.503605	12.867072
14.644751	786.793776	12.872090
14.639946	805.884198	12.877107
14.446932	792.456797	12.882125
14.208644	799.624595	12.887143
14.552087	805.065766	12.892160
14.074499	798.918562	12.897178
14.159651	801.000799	12.902195
14.207510	798.665728	12.907213
14.522972	801.050097	12.912231
14.204077	790.327341	12.917248
14.599104	800.061528	12.922266
14.467722	807.280843	12.927283
14.404876	799.806286	12.932301
14.369152	802.429855	12.937319
14.410235	800.953713	12.942336
14.261696	794.298776	12.947354
14.261553	798.668986	12.952371
14.361297	802.563820	12.957389
14.872815	808.672559	12.962407
14.477709	808.961287	12.967424
14.746070	799.943106	12.972442
14.512650	811.535051	12.977459
14.468673	785.199548	12.982477
14.594490	795.678284	12.987495
14.310231	805.996489	12.992512
14.674578	790.769828	12.997530
14.511080	803.431109	13.002547
14.653976	799.833228	13.007565
14.610566	789.702228	13.012583
14.489222	797.342240	13.017600
14.921711	790.025944	13.022618
14.456535	799.837628	13.027635
14.402014	794.102902	13.032653
14.696024	793.427225	13.037671
14.308487	796.282717	13.042688
14.651168	790.917999	13.047706
14.307735	801.904122	13.052723
14.595461	811.866344	13.057741
14.719493	808.783291	13.062759
14.561290	811.188958	13.067776
14.747030	818.271342	13.072794
14.606677	832.064729	13.077811
14.548153	831.597772	13.082829
14.863388	833.210182	13.087847
14.738816	827.559250	13.092864
14.847171	827.976454	13.097882
14.649351	834.271109	13.102899
14.821441	826.309866	13.107917
15.107150	833.429861	13.112935
14.727672	833.163650	13.117952
15.184449	828.758818	13.122970
14.648300	825.060585	13.127987
14.782762	831.212649	13.133005
14.880762	820.205961	13.138023
14.590597	826.075898	13.143040
14.878361	821.469414	13.148058
14.617431	839.976436	13.153075
14.992898	849.366806	13.158093
15.357335	846.603893	13.163111
15.347293	838.065277	13.168128
15.234401	812.323979	13.173146
14.910099	829.248454	13.178163
14.990187	819.547434	13.183181
15.098893	825.970335	13.188199
15.080960	829.547088	13.193216
15.405206	810.492423	13.198234
14.962092	819.726665	13.203251
15.339787	821.914371	13.208269
15.301941	818.025056	13.213287
15.219084	814.555306	13.218304
15.415575	818.107939	13.223322
14.997528	818.865823	13.228339
15.068521	816.884143	13.233357
15.180425	822.290171	13.238375
15.114661	829.281961	13.243392
15.384949	817.345596	13.248410
15.460964	824.500632	13.253427
15.569395	826.875426	13.258445
15.141532	813.321395	13.263463
15.381000	821.608549	13.268480
15.670168	820.298162	13.273498
15.625784	818.181640	13.278515
15.680799	825.577405	13.283533
15.505710	814.494513	13.288551
15.525290	813.382289	13.293568
15.492609	814.904581	13.298586
15.494692	820.527342	13.303603
15.586064	814.142732	13.308621
15.393549	809.048896	13.313639
15.391784	821.938732	13.318656
15.385418	821.385906	13.323674
15.308933	817.191322	13.328691
15.407969	823.754771	13.333709
15.515378	828.315936	13.338727
15.329767	820.736187	13.343744
15.879144	814.459911	13.348762
15.770501	819.917834	13.353779
15.583938	819.360836	13.358797
15.480546	813.354704	13.363815
15.720601	823.783288	13.368832
15.665312	825.429964	13.373850
15.455117	811.878441	13.378867
15.370015	821.698676	13.383885
15.792270	816.018396	13.388903
15.633800	815.477323	13.393920
15.856230	809.710503	13.398938
15.943562	816.782086	13.403955
15.685584	820.131134	13.408973
15.682585	819.580114	13.413991
15.682381	822.129227	13.419008
15.783796	818.548922	13.424026
15.789513	815.637262	13.429043
15.893083	807.994676	13.434061
15.994614	818.591296	13.439079
15.726071	820.723226	13.444096
15.769358	802.510124	13.449114
15.790859	808.855223	13.454131
15.715390	831.987595	13.459149
16.233515	825.380912	13.464167
15.695764	839.413960	13.469184
15.997656	837.643778	13.474202
15.957093	836.434818	13.479219
16.117027	831.745046	13.484237
16.066198	831.260186	13.489255
15.792996	830.243677	13.494272
15.956900	829.265544	13.499290
15.876020	834.442361	13.504307
16.191891	841.953954	13.509325
16.374576	850.316835	13.514343
16.213397	819.910952	13.519360
16.043977	814.590702	13.524378
16.345667	815.999089	13.529395
15.990532	812.335797	13.534413
15.794872	810.889329	13.539431
15.982723	828.170818	13.544448
16.172418	836.917204	13.549466
16.059833	841.489929	13.554483
15.880762	850.792642	13.559501
16.267590	843.610614	13.564519
16.294273	842.422326	13.569536
16.078141	850.943516	13.574554
16.097857	848.030520	13.579571
16.335353	836.342230	13.584589
16.735170	835.318321	13.589607
16.533153	851.157360	13.594624
16.302286	849.629027	13.599642
16.218262	846.331773	13.604659
15.955535	848.103462	13.609677
16.381751	839.293971	13.614695
15.914144	836.674461	13.619712
16.273705	849.914967	13.624730
16.251652	844.583442	13.629747
16.327216	842.853809	13.634765
16.268206	840.729270	13.639783
16.196289	853.217122	13.644800
16.331116	842.869758	13.649818
16.447220	833.620664	13.654835
16.090604	842.567646	13.659853
16.370590	857.404378	13.664871
16.856918	866.601865	13.669888
16.944592	858.326271	13.674906
16.780625	850.482644	13.679923
16.628586	829.512448	13.684941
16.839845	829.030135	13.689959
16.853304	823.318410	13.694976
16.441436	821.566789	13.699994
16.704045	829.082651	13.705011
16.521991	845.615006	13.710029
16.998017	821.940830	13.715047
16.668394	837.671931	13.720064
16.564126	836.819004	13.725082
16.650480	834.688845	13.730099
16.749459	841.818445	13.735117
16.989053	830.939011	13.740135
16.899575	833.353301	13.745152
16.474262	833.473825	13.750170
17.161579	834.618822	13.755187
16.635664	836.615070	13.760205
16.671020	833.130013	13.765223
16.480209	846.981939	13.770240
16.269669	837.940040	13.775258
17.129956	849.082332	13.780275
16.851207	873.213532	13.785293
17.430711	858.936106	13.790311
17.183403	849.781597	13.795328
16.887103	831.769138	13.800346
16.696168	837.516008	13.805363
16.485554	835.282099	13.810381
16.909857	837.188239	13.815399
17.314937	866.786777	13.820416
17.225450	872.723157	13.825434
16.841965	847.580448	13.830451
17.150697	858.416821	13.835469
17.148725	846.580138	13.840487
16.981263	847.064078	13.845504
16.850819	854.931170	13.850522
16.845843	851.315497	13.855539
16.786209	857.153057	13.860557
17.099438	858.783122	13.865575
17.044509	850.633833	13.870592
17.033752	862.474992	13.875610
17.577338	861.154835	13.880627
17.266952	860.815505	13.885645
17.495273	855.694031	13.890663
17.479121	861.357116	13.895680
17.316404	864.697221	13.900698
17.744679	858.514647	13.905715
17.578480	852.137650	13.910733
17.344042	828.108024	13.915751
17.223735	829.707877	13.920768
16.815275	826.778749	13.925786
17.309157	832.348486	13.930803
17.339105	848.699481	13.935821
17.537217	858.730272	13.940839
17.428432	857.543703	13.945856
17.081758	853.496791	13.950874
17.646158	847.433235	13.955891
17.671962	870.860584	13.960909
17.489951	865.796582	13.965927
17.545418	856.082976	13.970944
17.412513	858.588781	13.975962
17.321142	865.146515	13.980979
17.418473	861.376753	13.985997
17.769360	861.130373	13.991015
17.638668	862.834879	13.996032
17.299169	860.037826	14.001050
17.523273	855.564959	14.006067
17.045029	876.234606	14.011085
17.458944	859.114603	14.016103
17.366485	856.317369	14.021120
17.226533	862.324474	14.026138
17.670299	854.997034	14.031155
17.751012	857.268953	14.036173
17.627534	855.219226	14.041191
17.934542	871.220973	14.046208
17.217492	866.175518	14.051226
17.706790	855.727254	14.056243
17.703893	889.788400	14.061261
17.851448	885.995277	14.066279
18.262345	886.049945	14.071296
18.217597	884.323756	14.076314
18.214965	868.224863	14.081331
17.938310	868.927697	14.086349
17.837466	862.725294	14.091367
17.468616	864.209559	14.096384
16.991138	866.813441	14.101402
17.682593	866.795767	14.106419
17.595085	888.393787	14.111437
18.100566	885.163448	14.116455
18.183462	876.951416	14.121472
17.904820	886.085993	14.126490
18.172290	881.932959	14.131507
17.896256	881.056062	14.136525
18.318783	886.296728	14.141543
18.431840	884.057642	14.146560
18.030373	891.898294	14.151578
18.369458	895.502171	14.156595
17.796399	894.284861	14.161613
17.922341	884.643631	14.166631
18.106397	876.101358	14.171648
17.864090	883.928890	14.176666
18.568189	873.848587	14.181683
18.453507	878.088070	14.186701
18.324182	886.332089	14.191719
18.505342	880.583281	14.196736
18.104048	890.076255	14.201754
18.520967	873.352615	14.206771
17.837256	884.932823	14.211789
18.075513	877.676334	14.216807
18.064366	875.756045	14.221824
17.815898	889.090568	14.226842
18.118109	880.304793	14.231859
17.998766	881.877332	14.236877
18.116590	900.803244	14.241895
18.593000	905.101228	14.246912
18.609788	905.668973	14.251930
19.269206	901.733002	14.256947
18.814707	885.780403	14.261965
18.510004	876.985789	14.266983
18.668949	872.361905	14.272000
18.453153	885.313044	14.277018
18.511893	862.187202	14.282035
18.504252	866.118102	14.287053
18.212355	879.067543	14.292071
18.598453	865.504425	14.297088
18.435812	871.918063	14.302106
18.278105	873.725343	14.307123
18.802255	886.069749	14.312141
18.500503	880.300762	14.317159
18.752732	894.776732	14.322176
18.631095	908.117964	14.327194
18.712436	904.175374	14.332211
18.563331	911.928180	14.337229
18.467582	908.214522	14.342247
18.704308	904.874190	14.347264
18.736300	903.934974	14.352282
18.627948	912.777006	14.357299
18.634061	910.220906	14.362317
18.774134	901.816670	14.367335
18.975607	900.696523	14.372352
18.858565	912.339182	14.377370
18.972698	905.439252	14.382387
18.745552	907.040137	14.387405
18.377384	918.650986	14.392423
18.768178	903.395833	14.397440
18.735697	901.423172	14.402458
18.861484	914.983318	14.407475
18.977879	916.299326	14.412493
19.217049	928.713493	14.417511
19.481630	919.373977	14.422528
19.095159	910.869381	14.427546
19.109633	911.275038	14.432563
19.280388	900.240721	14.437581
18.968601	902.657415	14.442599
19.303905	893.970180	14.447616
19.285979	898.492837	14.452634
19.517183	893.792450	14.457651
19.327441	905.860329	14.462669
19.361864	901.078502	14.467687
19.598932	895.628169	14.472704
19.265238	899.020252	14.477722
19.339798	904.395185	14.482739
19.413715	904.205989	14.487757
19.717769	898.533009	14.492775
19.528788	893.500065	14.497792
19.583248	903.651851	14.502810
19.420164	886.333816	14.507827
19.220055	881.256660	14.512845
19.402179	881.544570	14.517863
19.290679	881.758682	14.522880
19.469981	891.266420	14.527898
19.685110	883.810244	14.532915
19.462719	876.927953	14.537933
19.384609	869.134290	14.542951
19.087193	870.986798	14.547968
19.408609	889.722586	14.552986
19.534253	893.772092	14.558003
19.731138	890.034780	14.563021
19.538608	897.875054	14.568039
19.528944	889.720036	14.573056
19.303266	892.603315	14.578074
19.466342	892.885320	14.583091
19.798537	897.363010	14.588109
19.554749	894.991391	14.593127
19.780474	882.484296	14.598144
19.197449	896.042190	14.603162
19.668042	894.645133	14.608179
19.358761	897.090638	14.613197
19.450784	913.006226	14.618215
19.715778	900.330058	14.623232
19.475116	901.834474	14.628250
19.311282	896.337124	14.633267
19.488311	910.883596	14.638285
19.735820	932.195255	14.643303
19.759561	916.167826	14.648320
19.940838	919.812646	14.653338
20.272375	929.914627	14.658355
20.146022	920.735167	14.663373
19.810977	927.289207	14.668391
20.068813	922.747077	14.673408
19.940524	925.433593	14.678426
19.852757	919.990285	14.683443
19.825577	912.857058	14.688461
19.538200	930.916772	14.693479
20.227024	921.026527	14.698496
20.098679	920.606924	14.703514
19.936282	926.807099	14.708531
20.079379	910.792819	14.713549
19.548646	923.902511	14.718567
19.988028	918.761785	14.723584
19.954871	922.119462	14.728602
20.132369	944.250041	14.733619
20.739538	945.326908	14.738637
20.262766	936.003021	14.743655
20.376056	921.610685	14.748672
20.229133	923.662994	14.753690
20.477510	922.130838	14.758707
20.655286	917.046332	14.763725
20.547866	914.427315	14.768743
20.334809	918.918751	14.773760
20.310534	919.185858	14.778778
20.325154	909.162983	14.783795
20.434155	909.881798	14.788813
20.044355	923.324041	14.793831
20.419406	905.133342	14.798848
20.488951	914.120354	14.803866
20.643632	915.003735	14.808883
20.825782	923.227891	14.813901
20.496249	930.199744	14.818919
20.789409	917.272398	14.823936
20.727435	922.189081	14.828954
20.867556	911.321403	14.833971
20.968801	909.119889	14.838989
20.426331	919.276546	14.844007
20.847910	916.551807	14.849024
20.580524	919.789656	14.854042
20.436127	919.291225	14.859059
20.466099	910.090564	14.864077
20.515393	912.282168	14.869095
20.501950	913.200712	14.874112
20.313755	923.722175	14.879130
20.466274	918.629837	14.884147
20.702442	917.733048	14.889165
20.803598	945.490280	14.894183
20.817006	951.019894	14.899200
20.976729	942.987420	14.904218
21.073816	946.130012	14.909235
20.878235	918.558536	14.914253
20.406842	928.994248	14.919271
20.940099	934.568341	14.924288
21.030017	936.290228	14.929306
20.864716	949.919764	14.934323
21.210807	949.297078	14.939341
20.860464	937.400100	14.944359
20.860205	937.322847	14.949376
21.248296	937.813294	14.954394
21.100652	945.742122	14.959411
21.099299	937.912516	14.964429
21.047525	941.408092	14.969447
21.148268	940.286382	14.974464
21.242954	938.133774	14.979482
20.872186	948.254203	14.984499
20.781195	945.302801	14.989517
20.663957	938.581025	14.994535
21.021405	942.439018	14.999552
20.656105	947.144365	15.004570
20.687717	944.550390	15.009587
21.052507	959.292809	15.014605
20.948479	962.059067	15.019623
21.676980	949.316301	15.024640
21.643237	944.949295	15.029658
21.490323	963.890994	15.034675
21.694833	951.157568	15.039693
21.512329	943.005694	15.044711
21.546149	949.823434	15.049728
21.649045	954.371409	15.054746
21.406727	951.841102	15.059763
21.989094	952.067597	15.064781
21.568329	945.117680	15.069799
21.621739	933.419586	15.074816
21.651905	929.506703	15.079834
21.590789	938.384538	15.084851
21.865096	922.606883	15.089869
21.705841	933.135182	15.094887
21.382442	927.939926	15.099904
21.428189	928.170171	15.104922
21.569139	925.616684	15.109939
21.768856	939.122713	15.114957
21.551968	950.213991	15.119975
21.451580	946.668383	15.124992
22.020417	953.041871	15.130010
21.828783	960.317663	15.135027
21.752163	942.449053	15.140045
21.720897	948.202939	15.145063
21.783374	948.283793	15.150080
21.766291	951.209666	15.155098
21.834924	949.300196	15.160115
22.023216	942.798452	15.165133
21.866978	943.172981	15.170151
22.222264	943.452844	15.175168
22.085977	948.685600	15.180186
21.593232	954.625079	15.185203
21.882804	942.830580	15.190221
21.768978	952.946637	15.195239
21.974675	952.449593	15.200256
22.114138	941.144483	15.205274
22.077455	947.452116	15.210291
22.027742	946.390204	15.215309
22.008705	955.147730	15.220327
22.076043	956.474997	15.225344
21.954476	953.598515	15.230362
21.942042	946.450436	15.235379
22.054962	953.353514	15.240397
21.833657	956.941959	15.245415
21.562964	955.619274	15.250432
22.124351	969.453486	15.255450
22.167649	982.166553	15.260467
22.132931	972.417982	15.265485
21.763452	972.288772	15.270503
21.955493	975.576674	15.275520
22.778274	970.067608	15.280538
22.366771	979.702850	15.285555
22.744935	968.446055	15.290573
22.597704	971.599897	15.295591
22.596362	966.145834	15.300608
22.617891	974.203682	15.305626
22.684159	976.993366	15.310643
22.767075	969.231300	15.315661
22.724268	967.434222	15.320679
22.592457	979.600146	15.325696
22.629471	970.256283	15.330714
22.388885	980.410722	15.335731
22.505065	975.995609	15.340749
22.627899	968.835007	15.345767
22.587668	971.587379	15.350784
22.708169	964.930814	15.355802
22.361930	973.127866	15.360819
22.926875	976.630080	15.365837
22.908679	984.432930	15.370855
22.984510	975.444888	15.375872
22.919043	969.702753	15.380890
22.379548	982.678435	15.385907
22.421780	971.968106	15.390925
22.842186	988.093534	15.395943
23.147523	990.373326	15.400960
23.418498	1000.860000	15.405978
22.991324	992.450848	15.410995
23.183543	976.014087	15.416013
23.282499	971.061760	15.421031
22.989836	969.211697	15.426048
23.274747	967.354363	15.431066
22.979375	972.797339	15.436083
23.126469	955.833702	15.441101
23.103273	963.555690	15.446119
23.026614	963.449141	15.451136
23.196396	963.782490	15.456154
23.003485	972.512765	15.461171
23.330018	963.410873	15.466189
23.147297	959.412612	15.471207
23.254456	961.490349	15.476224
23.631517	958.924506	15.481242
23.248770	961.350081	15.486259
23.239742	961.002279	15.491277
23.253935	970.925668	15.496295
23.055642	961.176090	15.501312
23.548194	971.499182	15.506330
23.022228	977.371141	15.511347
23.047484	981.695481	15.516365
23.668202	991.126598	15.521383
23.236575	995.363970	15.526400
23.529938	994.097060	15.531418
23.245486	994.478509	15.536435
23.322205	986.538454	15.541453
23.735791	986.684986	15.546471
23.629311	992.686315	15.551488
23.874133	984.266398	15.556506
23.512036	990.650556	15.561523
23.997870	977.343153	15.566541
23.798344	979.029131	15.571559
23.624677	984.756768	15.576576
23.758343	983.195637	15.581594
23.632814	979.781613	15.586611
23.604418	975.126955	15.591629
23.831975	993.505514	15.596647
23.388769	985.462631	15.601664
23.559015	980.309776	15.606682
23.812317	993.012553	15.611699
24.100152	1001.557908	15.616717
24.078437	986.940620	15.621735
23.378293	993.083254	15.626752
23.924751	990.790049	15.631770
23.793177	988.721174	15.636787
23.635350	989.905369	15.641805
23.865023	989.925529	15.646823
24.103227	1001.103127	15.651840
24.202931	1002.356263	15.656858
23.952501	1008.921941	15.661875
23.945596	1010.142113	15.666893
24.082942	1013.849520	15.671911
24.060528	1020.864839	15.676928
23.962298	1021.861661	15.681946
24.176183	1017.096394	15.686963
23.847715	1017.820097	15.691981
24.187242	1012.318349	15.696999
24.187468	1010.867636	15.702016
24.529931	1009.531401	15.707034
24.519190	1021.188657	15.712051
24.483572	1020.458407	15.717069
24.515153	1012.649497	15.722087
24.174692	1012.085349	15.727104
24.706566	1007.491022	15.732122
24.673658	1020.518628	15.737139
24.613330	1015.442341	15.742157
24.713702	1012.174805	15.747175
24.388446	1017.280965	15.752192
24.806986	1013.753900	15.757210
24.915721	1010.414622	15.762227
24.426291	992.180487	15.767245
24.704654	992.113482	15.772263
24.422034	996.095858	15.777280
24.440630	1008.278478	15.782298
24.628721	1015.802022	15.787315
24.707958	1016.646311	15.792333
24.769787	1005.588882	15.797351
24.592220	1017.861789	15.802368
24.789919	1020.237410	15.807386
24.647244	1016.964278	15.812403
24.794606	1014.748338	15.817421
25.076237	1010.367772	15.822439
24.581244	1015.236280	15.827456
24.587522	1010.197207	15.832474
24.871786	1010.439899	15.837491
24.470188	1008.409935	15.842509
24.887928	1010.241802	15.847527
24.560300	1025.958201	15.852544
24.738397	1017.524296	15.857562
25.042481	1016.444753	15.862579
25.234196	1039.690148	15.867597
25.247881	1033.476820	15.872615
24.947239	1019.787330	15.877632
24.828381	1019.980320	15.882650
25.261961	1029.074045	15.887667
25.296202	1030.950295	15.892685
25.620991	1022.424737	15.897703
25.361593	1021.999726	15.902720
25.083645	1017.626605	15.907738
24.991445	1002.627614	15.912755
25.190107	1026.351284	15.917773
25.435246	1022.400097	15.922791
25.460319	1031.786585	15.927808
25.280667	1027.440910	15.932826
25.358183	1025.152569	15.937843
25.287329	1019.915941	15.942861
25.493622	1026.335988	15.947879
25.172404	1040.314344	15.952896
25.630384	1027.271790	15.957914
25.605927	1024.304359	15.962931
25.608479	1034.799101	15.967949
25.791418	1030.672790	15.972967
25.642835	1030.288806	15.977984
25.749877	1024.411764	15.983002
25.762643	1009.862563	15.988019
25.334648	998.064279	15.993037
25.566011	1005.893015	15.998055
25.596941	1026.501848	16.003072
25.730257	1025.472469	16.008090
25.614505	1022.713495	16.013107
25.788057	1032.968894	16.018125
25.939055	1028.753684	16.023143
25.696482	1036.169599	16.028160
25.704935	1029.909311	16.033178
25.794203	1035.333622	16.038195
25.682940	1031.194914	16.043213
26.105922	1028.598248	16.048231
25.917054	1029.123913	16.053248
25.848515	1028.354130	16.058266
25.890510	1029.326599	16.063283
26.033832	1021.908990	16.068301
26.093887	1016.730834	16.073319
25.797250	1026.316420	16.078336
26.194955	1022.305185	16.083354
26.038990	1024.812269	16.088371
25.995496	1020.864790	16.093389
25.925885	1024.111113	16.098407
25.965372	1022.664441	16.103424
25.964313	1039.907321	16.108442
26.248774	1045.915512	16.113459
26.276371	1054.348515	16.118477
26.237133	1046.185015	16.123495
26.143083	1054.403614	16.128512
26.429508	1042.603654	16.133530
26.473540	1048.146449	16.138547
26.509905	1058.924743	16.143565
26.746198	1048.283554	16.148583
26.671370	1054.011219	16.153600
26.471075	1050.478652	16.158618
26.721930	1042.174221	16.163635
26.737251	1047.997302	16.168653
26.787006	1035.457854	16.173671
26.361017	1013.438673	16.178688
26.555805	1031.391470	16.183706
26.915310	1041.561332	16.188723
26.737630	1024.496985	16.193741
26.593488	1012.439222	16.198759
26.690056	1024.506133	16.203776
26.467279	1037.173762	16.208794
26.744274	1034.239865	16.213811
26.741314	1055.002146	16.218829
26.797750	1039.995384	16.223847
26.965947	1044.490673	16.228864
27.122622	1061.818712	16.233882
26.986456	1047.564019	16.238899
26.933154	1041.092120	16.243917
27.111582	1041.569883	16.248935
26.777552	1041.461974	16.253952
26.389528	1038.633444	16.258970
26.639639	1044.535913	16.263987
26.196153	1051.897256	16.269005
26.236100	1045.765789	16.274023
26.542779	1062.130621	16.279040
26.786401	1065.264769	16.284058
27.027613	1069.179495	16.289075
26.961515	1068.379194	16.294093
27.188299	1070.870468	16.299111
27.157159	1074.998087	16.304128
27.360956	1070.371356	16.309146
27.737070	1064.310489	16.314163
27.556951	1080.286870	16.319181
27.427101	1077.673696	16.324199
27.456032	1068.615705	16.329216
27.408424	1067.869425	16.334234
27.620719	1066.795599	16.339251
27.541776	1071.261669	16.344269
27.547570	1058.982867	16.349287
27.362015	1066.289096	16.354304
27.035808	1069.958474	16.359322
27.287659	1064.930959	16.364339
27.126407	1075.606904	16.369357
27.429275	1058.513592	16.374375
27.412862	1065.048790	16.379392
27.602886	1083.364282	16.384410
27.760136	1079.248107	16.389427
27.474757	1099.682182	16.394445
27.906557	1095.853254	16.399463
28.581811	1094.452572	16.404480
27.970388	1079.061731	16.409498
27.678322	1059.069609	16.414515
27.832921	1059.129238	16.419533
28.124985	1051.868695	16.424551
27.905213	1062.691484	16.429568
27.845597	1065.626768	16.434586
28.243248	1056.919790	16.439603
27.866054	1067.023744	16.444621
27.855878	1064.108660	16.449639
27.719104	1049.976584	16.454656
27.969049	1058.684307	16.459674
28.267257	1069.866900	16.464691
28.222629	1073.856023	16.469709
27.688867	1066.477064	16.474727
27.998408	1075.797775	16.479744
28.162550	1096.327711	16.484762
28.121443	1080.150322	16.489779
28.229092	1097.757126	16.494797
28.282503	1092.918273	16.499815
28.432692	1092.322739	16.504832
28.043877	1101.055248	16.509850
28.270225	1088.259841	16.514867
28.245051	1090.525281	16.519885
28.415985	1086.729229	16.524903
28.534735	1088.952975	16.529920
28.376113	1093.887259	16.534938
28.712964	1089.104307	16.539955
28.469030	1094.909432	16.544973
28.384021	1082.727590	16.549991
28.526792	1090.820966	16.555008
28.085795	1094.884353	16.560026
28.309776	1089.980706	16.565043
28.431970	1088.262236	16.570061
28.386291	1116.650237	16.575079
28.876007	1112.315362	16.580096
29.255630	1116.094157	16.585114
29.240318	1098.314135	16.590131
29.582836	1082.234739	16.595149
29.324649	1079.010499	16.600167
29.507503	1075.815919	16.605184
29.262840	1071.717746	16.610202
29.220016	1056.705424	16.615219
28.968268	1044.683230	16.620237
29.070465	1045.512409	16.625255
28.905672	1030.129687	16.630272
28.663301	1033.406923	16.635290
28.960978	1054.964553	16.640307
29.211510	1062.626399	16.645325
29.125189	1060.406851	16.650343
29.124762	1064.251881	16.655360
29.451314	1068.058033	16.660378
29.134168	1045.391893	16.665395
29.067678	1049.968380	16.670413
28.972637	1061.281195	16.675431
29.460895	1060.592204	16.680448
29.338322	1076.298093	16.685466
29.372037	1071.316758	16.690483
29.446460	1069.569478	16.695501
29.373277	1067.221697	16.700519
29.833688	1078.582575	16.705536
28.959267	1064.689781	16.710554
29.589098	1055.561432	16.715571
29.196075	1075.291538	16.720589
29.037517	1070.558770	16.725607
29.468577	1069.929026	16.730624
29.095206	1070.887474	16.735642
29.644018	1066.970036	16.740659
29.617163	1067.953688	16.745677
29.400196	1071.972569	16.750695
29.723894	1069.099736	16.755712
29.364811	1076.478830	16.760730
29.629039	1075.830895	16.765747
29.967476	1098.315352	16.770765
29.452604	1105.369575	16.775783
30.117103	1100.816089	16.780800
29.734955	1107.414399	16.785818
29.656330	1098.958022	16.790835
29.688959	1099.450039	16.795853
29.653718	1114.575391	16.800871
30.009564	1104.780500	16.805888
29.804824	1102.712776	16.810906
29.819556	1086.141966	16.815923
29.853299	1102.010895	16.820941
29.758040	1105.677839	16.825959
30.010835	1119.482981	16.830976
29.796903	1121.933332	16.835994
30.125703	1127.119307	16.841011
29.898167	1133.913105	16.846029
30.548529	1121.753980	16.851047
30.897669	1129.298991	16.856064
30.350841	1131.337700	16.861082
30.344078	1129.472060	16.866099
30.388275	1128.386251	16.871117
30.391881	1133.138254	16.876135
30.258267	1132.077695	16.881152
30.305424	1123.635945	16.886170
30.516782	1117.129135	16.891187
30.470890	1122.235712	16.896205
30.404852	1127.083262	16.901223
30.699028	1111.843770	16.906240
30.603092	1124.988950	16.911258
30.570900	1137.409160	16.916275
30.653984	1126.845882	16.921293
30.568265	1129.455332	16.926311
30.460646	1125.214636	16.931328
30.339869	1132.136829	16.936346
30.454617	1125.753246	16.941363
30.483800	1134.017751	16.946381
30.435967	1154.027473	16.951399
30.667679	1148.420679	16.956416
30.943944	1152.025847	16.961434
31.064964	1155.757046	16.966451
31.031685	1159.616681	16.971469
31.181356	1158.534893	16.976487
31.191602	1150.035853	16.981504
31.570625	1146.278419	16.986522
31.058471	1140.914807	16.991539
31.254409	1127.947650	16.996557
30.821326	1128.143068	17.001575
31.146770	1129.007100	17.006592
31.388781	1135.867967	17.011610
31.068536	1140.699272	17.016627
31.671598	1144.230359	17.021645
31.241543	1141.590319	17.026663
31.489388	1132.434610	17.031680
31.447261	1126.411932	17.036698
31.384597	1125.828937	17.041715
31.172072	1116.097061	17.046733
31.302690	1123.945851	17.051751
31.652685	1142.958283	17.056768
31.391005	1146.297876	17.061786
31.527062	1134.742343	17.066803
31.803684	1145.942828	17.071821
31.652200	1147.555049	17.076839
31.653240	1135.938572	17.081856
31.509124	1141.539260	17.086874
31.761196	1136.665202	17.091891
31.878953	1140.397331	17.096909
31.465154	1138.486372	17.101927
31.423994	1144.875423	17.106944
31.601401	1140.846241	17.111962
31.248653	1141.333253	17.116979
31.368481	1135.546954	17.121997
31.416515	1164.534219	17.127015
31.748669	1172.937035	17.132032
31.668855	1179.678297	17.137050
32.136639	1185.300501	17.142067
32.221526	1169.774724	17.147085
32.098609	1173.716879	17.152103
32.298557	1180.832708	17.157120
31.859650	1169.592597	17.162138
31.757107	1167.865987	17.167155
32.385827	1170.005867	17.172173
32.214991	1169.676533	17.177191
32.712395	1158.495056	17.182208
32.756026	1166.241529	17.187226
32.841280	1177.753536	17.192243
32.563942	1166.694370	17.197261
32.432767	1162.893114	17.202279
32.688398	1138.274522	17.207296
32.572021	1138.847257	17.212314
32.526400	1133.811996	17.217331
32.623041	1123.923728	17.222349
32.284168	1137.836500	17.227367
32.315378	1124.049859	17.232384
32.343134	1138.784181	17.237402
32.673088	1158.179407	17.242419
32.830975	1154.221939	17.247437
32.773945	1163.921927	17.252455
32.710763	1152.320184	17.257472
32.694205	1162.104019	17.262490
32.759734	1151.984497	17.267507
32.931991	1163.416181	17.272525
33.065957	1167.949048	17.277543
32.940071	1155.177152	17.282560
32.531254	1147.148674	17.287578
32.643618	1158.733929	17.292595
32.403610	1151.404007	17.297613
32.368300	1154.830584	17.302631
32.625180	1150.011427	17.307648
32.954129	1151.471238	17.312666
33.002199	1162.221789	17.317683
33.225630	1165.499330	17.322701
33.310823	1182.526182	17.327719
32.920976	1165.371660	17.332736
33.211522	1171.269367	17.337754
33.264683	1183.238377	17.342771
33.666882	1176.909814	17.347789
33.314283	1187.851572	17.352807
33.328172	1180.692243	17.357824
33.613865	1177.516273	17.362842
33.274744	1191.321474	17.367859
33.552770	1184.768979	17.372877
33.349390	1181.591950	17.377895
33.384513	1193.299032	17.382912
33.634323	1184.679493	17.387930
33.735399	1184.022004	17.392947
34.028170	1199.468962	17.397965
33.797303	1189.929212	17.402983
33.503404	1177.324409	17.408000
33.671774	1178.856027	17.413018
33.502424	1182.175647	17.418035
33.231836	1185.129776	17.423053
33.591574	1186.835447	17.428071
33.502691	1194.396189	17.433088
33.364402	1192.919341	17.438106
33.362867	1192.062505	17.443123
33.717799	1205.197017	17.448141
33.879752	1214.697885	17.453159
33.942655	1213.501713	17.458176
34.153055	1210.525745	17.463194
33.811690	1210.824098	17.468211
34.530178	1212.218167	17.473229
34.256498	1212.678339	17.478247
34.250356	1206.999035	17.483264
34.502854	1206.430481	17.488282
34.103151	1212.659357	17.493299
34.505613	1204.979385	17.498317
34.582302	1207.776345	17.503335
34.211285	1210.894098	17.508352
34.645567	1202.052955	17.513370
34.210747	1206.940018	17.518387
34.812693	1196.229348	17.523405
34.527452	1200.489034	17.528423
34.754477	1195.452392	17.533440
34.647238	1200.997802	17.538458
34.566080	1205.466049	17.543475
34.853974	1194.173522	17.548493
34.738865	1203.669388	17.553511
34.791862	1187.018930	17.558528
34.989397	1177.060421	17.563546
34.630221	1178.504244	17.568563
34.466248	1166.815029	17.573581
34.403625	1187.381280	17.578599
34.796580	1190.916396	17.583616
35.320764	1202.650131	17.588634
34.850392	1205.895701	17.593651
34.615989	1191.663799	17.598669
34.539919	1204.053525	17.603687
34.798677	1207.877508	17.608704
34.713235	1200.174440	17.613722
34.631442	1207.041612	17.618739
34.621548	1200.986811	17.623757
34.859207	1221.307653	17.628775
35.030615	1233.709451	17.633792
35.127002	1224.207319	17.638810
35.293514	1232.065979	17.643827
35.006213	1232.268995	17.648845
35.333543	1233.158702	17.653863
35.196939	1230.881504	17.658880
35.580921	1230.151087	17.663898
35.274373	1241.491113	17.668915
35.533828	1225.120029	17.673933
35.360088	1225.677053	17.678951
35.292712	1221.704635	17.683968
35.578941	1226.492430	17.688986
35.470039	1235.036460	17.694003
35.460257	1222.910765	17.699021
35.289894	1235.097826	17.704039
35.521479	1248.035666	17.709056
35.857228	1249.249915	17.714074
35.716286	1253.065759	17.719091
35.880504	1252.918026	17.724109
36.013023	1256.936280	17.729127
35.706573	1252.496749	17.734144
36.313701	1245.425943	17.739162
36.207439	1250.286674	17.744179
36.251878	1246.603203	17.749197
36.075944	1233.896196	17.754215
35.626807	1222.987407	17.759232
36.193372	1236.064929	17.764250
36.021240	1251.411431	17.769267
36.195717	1248.159744	17.774285
36.183289	1247.540101	17.779303
36.020802	1255.767853	17.784320
36.280893	1251.355352	17.789338
36.196704	1259.297376	17.794355
36.251403	1249.320502	17.799373
36.349658	1246.558500	17.804391
36.059541	1247.355980	17.809408
36.123945	1243.887089	17.814426
36.332201	1246.237974	17.819443
36.601410	1231.039689	17.824461
36.457361	1238.925070	17.829479
36.622832	1248.203563	17.834496
36.993144	1246.339366	17.839514
36.596404	1245.357314	17.844531
36.535682	1247.570393	17.849549
36.629130	1249.061258	17.854567
36.759638	1254.372943	17.859584
36.861819	1256.349885	17.864602
36.925791	1270.602441	17.869619
36.684852	1275.839119	17.874637
36.424508	1269.007108	17.879655
36.703553	1270.807408	17.884672
37.049483	1251.495701	17.889690
37.300184	1269.925780	17.894707
37.097966	1271.839067	17.899725
37.445844	1260.582832	17.904743
37.105285	1274.164759	17.909760
37.433877	1260.387900	17.914778
37.024816	1262.123393	17.919795
37.055465	1270.561915	17.924813
37.301000	1264.919335	17.929831
37.287321	1265.556587	17.934848
37.129075	1255.872139	17.939866
36.866889	1254.543100	17.944883
36.911392	1250.762783	17.949901
37.017276	1258.772398	17.954919
37.083870	1274.953743	17.959936
37.607623	1274.909563	17.964954
37.675921	1274.473791	17.969971
37.288156	1289.717009	17.974989
37.592871	1278.624955	17.980007
37.564379	1284.638802	17.985024
37.909825	1280.418849	17.990042
37.785133	1292.786764	17.995059
37.500405	1282.704172	18.000077
37.620601	1279.077652	18.005095
37.458529	1280.933134	18.010112
37.801462	1283.869351	18.015130
37.743492	1288.451487	18.020147
37.752540	1296.761724	18.025165
37.924168	1286.186855	18.030183
37.891240	1285.365118	18.035200
38.068617	1308.346798	18.040218
38.090862	1306.231498	18.045235
38.067502	1303.034143	18.050253
38.238623	1317.153503	18.055271
38.487804	1313.165359	18.060288
38.921018	1297.506117	18.065306
38.602614	1277.196458	18.070323
38.724263	1267.700753	18.075341
38.466258	1260.990386	18.080359
38.287939	1265.130469	18.085376
38.247124	1259.031551	18.090394
38.315381	1258.179908	18.095411
38.451991	1266.689486	18.100429
38.776811	1256.878370	18.105447
38.586960	1248.983705	18.110464
38.716449	1251.535372	18.115482
38.574396	1266.281738	18.120499
38.555103	1259.633681	18.125517
38.771219	1274.005564	18.130535
38.983933	1286.991627	18.135552
38.985622	1297.679870	18.140570
38.929065	1292.304292	18.145587
38.792424	1301.721703	18.150605
38.855793	1292.964829	18.155623
38.650053	1293.831426	18.160640
39.186071	1292.277780	18.165658
39.240199	1300.553212	18.170675
39.025636	1295.488344	18.175693
38.844419	1300.190244	18.180711
38.783878	1292.079142	18.185728
39.003901	1293.831924	18.190746
38.839743	1303.631383	18.195763
39.047606	1298.767336	18.200781
39.217481	1287.021286	18.205799
38.939551	1308.902604	18.210816
39.148180	1322.496561	18.215834
39.695794	1324.431200	18.220851
39.612766	1317.373243	18.225869
39.817304	1325.841909	18.230887
39.637021	1317.644888	18.235904
40.130497	1311.808588	18.240922
39.748306	1306.476581	18.245939
39.727300	1284.400321	18.250957
39.539158	1280.932610	18.255975
39.428955	1304.202712	18.260992
39.679868	1302.857964	18.266010
39.674524	1320.533099	18.271027
39.641902	1320.683402	18.276045
39.923295	1307.289439	18.281063
39.512734	1317.988348	18.286080
39.879628	1314.293696	18.291098
40.068393	1307.582107	18.296115
39.839439	1316.505806	18.301133
39.820658	1315.143035	18.306151
39.914313	1319.193511	18.311168
39.832147	1313.701704	18.316186
39.900040	1325.524713	18.321203
39.888502	1338.707302	18.326221
40.039103	1340.534740	18.331239
39.970303	1350.839257	18.336256
40.510001	1335.581606	18.341274
40.565806	1332.543774	18.346291
40.223614	1348.110767	18.351309
40.423859	1335.651307	18.356327
40.222688	1340.120136	18.361344
40.271133	1338.502393	18.366362
40.149682	1338.141866	18.371379
40.391307	1358.209124	18.376397
41.173362	1359.830659	18.381415
41.187349	1361.774756	18.386432
41.402933	1347.608682	18.391450
41.386928	1331.990374	18.396467
40.943397	1326.922788	18.401485
41.408182	1316.871018	18.406503
41.075184	1330.309247	18.411520
40.891107	1328.975561	18.416538
40.757987	1331.140782	18.421555
40.920823	1328.308655	18.426573
40.969259	1324.633165	18.431591
40.932317	1326.541979	18.436608
41.131087	1332.747192	18.441626
41.148612	1325.023700	18.446643
41.250323	1319.900852	18.451661
41.213932	1329.269239	18.456679
41.258447	1328.184151	18.461696
41.107631	1331.482436	18.466714
41.241717	1343.659621	18.471731
41.256800	1367.868024	18.476749
41.792756	1354.618343	18.481767
41.514067	1366.159140	18.486784
41.438734	1364.190056	18.491802
41.579988	1357.053686	18.496819
41.732138	1362.757244	18.501837
41.756271	1366.715301	18.506855
41.717185	1361.026032	18.511872
41.785745	1360.354621	18.516890
41.719738	1364.352372	18.521907
41.975583	1359.366614	18.526925
42.213968	1347.340932	18.531943
41.765780	1354.588941	18.536960
41.576874	1349.404282	18.541978
42.122374	1350.247710	18.546995
41.545359	1348.044846	18.552013
41.941907	1347.595768	18.557031
41.997516	1351.873175	18.562048
42.081956	1360.637255	18.567066
42.198967	1379.069285	18.572083
41.923959	1380.884198	18.577101
42.157068	1385.784940	18.582119
42.399560	1381.572918	18.587136
42.530055	1387.230662	18.592154
42.493328	1385.464612	18.597171
42.355217	1389.927365	18.602189
42.599326	1380.714261	18.607207
42.619233	1372.571124	18.612224
42.580159	1370.851520	18.617242
42.614686	1371.980930	18.622259
42.402113	1379.365383	18.627277
42.717691	1371.606786	18.632295
42.547497	1380.975862	18.637312
42.125878	1370.934924	18.642330
42.723544	1372.333426	18.647347
42.798101	1378.685739	18.652365
42.503484	1391.708687	18.657383
42.946837	1389.412782	18.662400
43.077598	1395.306670	18.667418
43.536061	1399.149662	18.672435
43.001921	1398.012182	18.677453
43.471172	1400.343384	18.682471
43.444104	1397.179687	18.687488
43.191360	1390.302081	18.692506
43.077492	1363.934225	18.697523
43.106949	1384.547523	18.702541
43.324607	1393.241780	18.707559
43.497718	1401.323419	18.712576
43.463706	1392.571952	18.717594
43.869290	1401.569164	18.722611
43.673584	1415.934244	18.727629
43.831467	1393.016972	18.732647
43.371269	1395.007151	18.737664
43.367278	1393.566547	18.742682
43.888474	1391.524077	18.747699
43.498243	1395.649811	18.752717
43.742018	1394.442435	18.757735
43.559401	1393.282490	18.762752
43.713226	1397.248253	18.767770
44.064616	1397.918673	18.772787
43.659739	1400.148099	18.777805
44.019970	1391.728472	18.782823
43.643771	1390.863076	18.787840
43.988481	1412.179320	18.792858
44.057220	1397.362174	18.797875
43.927597	1390.237681	18.802893
44.018367	1404.406221	18.807911
43.974281	1420.807554	18.812928
44.421663	1423.579119	18.817946
44.806006	1412.763728	18.822963
44.292424	1413.330270	18.827981
44.564818	1423.951036	18.832999
44.550370	1413.309992	18.838016
44.626534	1417.070318	18.843034
44.769374	1415.829234	18.848051
44.300145	1414.912290	18.853069
44.569800	1408.946625	18.858087
44.550671	1411.460289	18.863104
44.374003	1409.101705	18.868122
44.565626	1410.510822	18.873139
44.522496	1424.985126	18.878157
44.648136	1414.233937	18.883175
44.721745	1414.687111	18.888192
44.553314	1432.387552	18.893210
44.709326	1434.158802	18.898227
45.181174	1430.648914	18.903245
44.837751	1447.748463	18.908263
45.151092	1436.048070	18.913280
45.091838	1440.976476	18.918298
45.251195	1433.851447	18.923315
45.221804	1439.790318	18.928333
45.419954	1441.041098	18.933351
45.466605	1436.881303	18.938368
44.850671	1450.880488	18.943386
45.339634	1438.666105	18.948403
45.428392	1439.773766	18.953421
45.343364	1444.993594	18.958439
45.623931	1453.283454	18.963456
45.534211	1446.790239	18.968474
45.654497	1455.159334	18.973491
45.522315	1474.720488	18.978509
45.742477	1475.957400	18.983527
46.055779	1463.520289	18.988544
45.724271	1468.307894	18.993562
45.803948	1473.444420	18.998579
46.196806	1478.284350	19.003597
45.874926	1467.046921	19.008615
46.222395	1475.099787	19.013632
45.761618	1477.797646	19.018650
46.320884	1466.257744	19.023667
46.046313	1472.504623	19.028685
46.305862	1482.334952	19.033703
46.290696	1473.261670	19.038720
46.066729	1459.461786	19.043738
46.246015	1464.571222	19.048755
45.959014	1477.848457	19.053773
45.677339	1464.554292	19.058791
45.644558	1471.642189	19.063808
46.051086	1499.154912	19.068826
46.336104	1493.843077	19.073843
46.568952	1493.566302	19.078861
46.633217	1499.246054	19.083879
46.768551	1498.693702	19.088896
46.582678	1502.940790	19.093914
46.912742	1493.182586	19.098931
46.679529	1492.911970	19.103949
46.643032	1490.157824	19.108967
47.069071	1489.068726	19.113984
46.805422	1503.171335	19.119002
46.891531	1504.944303	19.124019
46.984150	1508.657451	19.129037
47.082975	1526.416775	19.134055
47.504735	1518.094968	19.139072
47.637838	1518.051572	19.144090
47.479831	1506.237311	19.149107
47.408350	1497.789373	19.154125
47.178522	1500.683685	19.159143
47.471602	1493.049200	19.164160
47.506094	1517.202276	19.169178
47.555980	1501.441037	19.174195
47.537331	1515.987158	19.179213
47.123636	1505.724971	19.184231
47.779639	1512.872074	19.189248
47.600282	1528.140923	19.194266
47.713782	1514.254717	19.199283
47.566835	1513.277424	19.204301
47.260347	1514.444105	19.209319
47.355384	1506.838206	19.214336
47.622655	1514.063915	19.219354
48.105003	1541.233917	19.224371
48.162881	1535.696057	19.229389
48.230479	1529.626550	19.234407
48.528116	1507.114299	19.239424
48.286483	1508.114576	19.244442
48.176610	1494.668981	19.249459
48.460264	1495.576354	19.254477
48.303735	1504.171114	19.259495
48.287227	1502.872311	19.264512
48.176189	1502.677554	19.269530
48.443602	1504.584908	19.274547
48.354536	1501.246226	19.279565
48.259930	1527.994887	19.284583
48.436043	1531.375785	19.289600
48.571868	1538.535640	19.294618
48.466267	1541.586571	19.299635
48.856287	1530.636124	19.304653
48.474553	1527.772115	19.309671
48.803224	1528.266007	19.314688
48.394821	1539.011162	19.319706
48.796803	1529.715196	19.324723
48.350192	1523.860762	19.329741
48.503953	1548.029212	19.334759
49.099178	1546.780282	19.339776
49.055581	1557.653526	19.344794
49.163804	1557.665612	19.349811
49.389008	1547.600732	19.354829
49.247810	1550.512292	19.359847
49.453080	1548.318887	19.364864
49.395281	1550.243182	19.369882
49.605708	1552.838997	19.374899
49.677308	1552.511515	19.379917
49.645993	1548.923155	19.384935
49.809484	1539.688244	19.389952
49.465775	1531.525789	19.394970
49.450155	1537.814341	19.399987
49.689008	1540.409000	19.405005
49.517777	1542.565589	19.410023
49.922258	1545.917414	19.415040
49.622390	1542.152992	19.420058
49.864494	1543.330976	19.425075
49.818462	1542.580476	19.430093
49.425073	1549.395761	19.435111
49.788795	1543.521572	19.440128
49.807904	1548.393172	19.445146
49.773697	1557.162405	19.450163
50.015784	1566.660682	19.455181
50.173084	1587.862096	19.460199
50.166835	1575.325163	19.465216
50.129190	1584.038492	19.470234
50.015341	1589.536519	19.475251
50.245763	1576.352883	19.480269
50.151596	1593.661566	19.485287
50.301444	1581.332069	19.490304
50.362659	1589.401986	19.495322
50.687600	1603.207846	19.500339
50.548114	1596.665319	19.505357
51.079008	1604.687156	19.510375
50.942873	1601.041115	19.515392
50.730053	1582.624561	19.520410
50.565994	1594.012550	19.525427
50.916436	1596.139628	19.530445
51.048651	1596.329614	19.535463
50.996881	1593.903716	19.540480
50.566031	1596.860590	19.545498
50.817266	1586.917153	19.550515
51.090201	1592.109371	19.555533
51.062695	1609.067733	19.560551
51.045106	1584.842347	19.565568
51.075618	1602.744132	19.570586
51.192486	1614.542935	19.575603
51.497812	1615.323129	19.580621
51.294411	1624.904307	19.585639
51.613312	1620.429629	19.590656
51.727239	1622.489312	19.595674
51.495742	1632.688243	19.600691
51.645528	1632.417516	19.605709
51.629239	1639.079593	19.610727
51.978595	1634.720925	19.615744
51.872178	1627.519859	19.620762
51.486538	1619.877012	19.625779
51.591133	1620.602199	19.630797
51.533486	1625.964395	19.635815
51.675530	1622.588283	19.640832
51.880025	1638.163248	19.645850
51.910895	1639.572969	19.650867
52.244876	1632.030463	19.655885
51.859159	1650.661821	19.660903
51.819385	1647.127782	19.665920
52.134993	1645.729801	19.670938
52.555413	1647.433567	19.675955
52.632412	1634.460052	19.680973
52.509203	1639.622091	19.685991
52.522361	1642.185567	19.691008
52.510528	1642.415694	19.696026
52.221767	1633.141302	19.701043
52.675483	1644.214870	19.706061
52.525531	1647.145413	19.711079
52.779295	1640.871106	19.716096
52.933866	1649.303334	19.721114
52.673441	1672.066014	19.726131
53.002159	1666.439066	19.731149
52.869800	1665.683929	19.736167
53.139419	1666.013985	19.741184
53.096674	1668.577060	19.746202
53.158954	1669.452923	19.751219
53.514285	1665.616418	19.756237
53.203363	1674.761321	19.761255
53.272608	1666.678961	19.766272
53.409056	1657.268354	19.771290
52.849999	1676.129737	19.776307
53.281011	1661.469374	19.781325
53.443630	1655.793312	19.786343
53.353989	1661.456633	19.791360
53.455399	1665.733645	19.796378
53.224494	1662.431553	19.801395
53.775398	1678.431733	19.806413
53.721262	1695.542012	19.811431
53.912945	1693.205970	19.816448
54.146345	1690.193438	19.821466
53.545736	1687.307897	19.826483
53.833618	1701.123709	19.831501
54.216870	1687.686407	19.836519
53.977720	1678.371313	19.841536
54.210926	1680.278831	19.846554
54.083902	1688.027394	19.851571
54.445342	1678.926006	19.856589
54.284015	1682.021208	19.861607
54.384704	1687.869987	19.866624
54.750212	1682.175939	19.871642
54.144620	1672.320497	19.876659
54.364332	1677.925029	19.881677
54.386636	1686.251394	19.886695
54.535968	1702.942283	19.891712
54.502550	1707.324253	19.896730
54.405497	1707.148834	19.901747
54.701099	1701.294305	19.906765
54.835173	1713.667824	19.911783
55.099375	1708.014519	19.916800
55.062867	1707.028412	19.921818
54.789261	1717.853962	19.926835
55.041389	1700.026491	19.931853
55.197865	1700.151454	19.936871
55.500992	1708.262748	19.941888
55.516766	1715.636199	19.946906
55.156949	1702.830662	19.951923
55.161329	1689.821468	19.956941
55.111030	1710.209240	19.961959
55.057140	1707.962588	19.966976
55.497402	1710.720425	19.971994
55.162290	1734.338932	19.977011
55.403078	1720.135285	19.982029
55.562704	1725.218336	19.987047
55.858450	1735.420553	19.992064
55.981673	1727.387699	19.997082
55.432848	1733.924655	20.002099
55.552124	1724.851841	20.007117
55.529146	1735.907016	20.012135
55.590157	1727.699032	20.017152
55.927812	1743.474119	20.022170
55.962775	1764.045288	20.027187
56.205177	1747.079891	20.032205
56.103984	1755.728040	20.037223
56.096971	1758.864875	20.042240
56.725902	1757.472188	20.047258
56.368791	1754.760740	20.052275
56.450210	1761.891703	20.057293
56.560392	1759.420909	20.062311
56.824300	1760.279796	20.067328
56.928531	1765.548566	20.072346
56.608817	1761.526576	20.077363
56.910731	1758.558214	20.082381
56.652303	1759.782119	20.087399
56.658690	1767.660232	20.092416
56.507611	1757.936295	20.097434
56.433749	1764.573693	20.102451
56.514345	1753.651191	20.107469
56.636769	1761.823865	20.112487
56.528385	1780.410535	20.117504
57.108621	1781.336626	20.122522
56.879289	1789.521187	20.127539
56.768713	1793.243968	20.132557
57.108066	1781.884052	20.137575
56.906182	1800.164780	20.142592
57.443811	1809.018775	20.147610
57.426727	1802.688976	20.152627
57.579580	1805.915334	20.157645
57.733546	1809.367465	20.162663
58.234433	1798.124527	20.167680
58.474528	1800.132287	20.172698
58.561797	1796.487271	20.177715
58.346548	1768.336093	20.182733
58.094024	1767.471100	20.187751
57.959948	1765.642363	20.192768
58.139382	1760.497275	20.197786
58.270285	1761.089201	20.202803
58.432506	1762.404010	20.207821
58.598672	1753.595442	20.212839
58.328411	1763.491259	20.217856
58.282072	1748.368030	20.222874
58.254289	1759.045914	20.227891
58.510148	1761.415388	20.232909
58.576751	1771.855273	20.237927
58.617453	1768.259095	20.242944
58.531200	1759.851638	20.247962
58.576792	1768.786523	20.252979
58.684551	1768.393030	20.257997
58.712026	1744.638822	20.263015
58.252855	1761.602746	20.268032
58.283843	1770.172572	20.273050
58.415482	1782.411330	20.278067
58.540586	1780.622626	20.283085
58.537714	1792.957822	20.288103
58.726096	1814.616167	20.293120
58.877361	1805.572267	20.298138
58.864131	1826.265052	20.303155
58.367983	1828.425772	20.308173
58.558596	1829.316261	20.313191
58.804317	1849.120524	20.318208
59.815488	1841.911433	20.323226
59.600347	1849.805527	20.328243
59.789952	1841.695313	20.333261
59.889782	1842.789758	20.338279
60.081663	1839.685841	20.343296
60.395984	1838.346514	20.348314
60.110164	1822.521340	20.353331
60.133676	1814.820625	20.358349
60.396561	1808.303632	20.363367
59.860008	1805.796608	20.368384
60.117596	1803.316605	20.373402
60.378101	1810.456378	20.378419
59.902953	1811.102002	20.383437
60.154353	1807.469621	20.388455
59.864729	1809.053562	20.393472
59.861555	1810.840532	20.398490
60.181178	1833.849094	20.403507
60.054520	1837.368663	20.408525
60.505231	1840.266119	20.413543
60.439978	1841.354579	20.418560
60.221537	1833.509410	20.423578
60.282079	1852.814619	20.428595
60.023104	1863.953366	20.433613
60.768938	1861.889661	20.438631
60.536975	1868.309754	20.443648
60.982573	1873.531994	20.448666
61.059390	1863.712071	20.453683
60.917263	1856.849041	20.458701
61.174870	1843.176099	20.463719
61.010007	1854.968694	20.468736
61.393990	1848.742660	20.473754
61.505123	1852.652020	20.478771
61.495762	1852.805570	20.483789
61.749091	1854.389746	20.488807
61.463866	1855.845815	20.493824
61.427094	1845.685268	20.498842
61.502432	1851.985489	20.503859
61.568209	1869.740436	20.508877
62.203403	1876.118803	20.513895
61.904941	1869.392612	20.518912
61.972973	1856.453064	20.523930
61.968161	1853.063970	20.528947
62.059708	1859.850236	20.533965
62.188488	1867.171428	20.538983
62.127558	1879.577698	20.544000
62.289851	1865.474082	20.549018
62.398786	1869.365112	20.554035
62.456508	1879.225111	20.559053
62.499843	1872.119839	20.564071
62.276937	1866.728246	20.569088
62.208252	1876.686484	20.574106
62.223001	1877.797549	20.579123
61.952141	1879.500035	20.584141
62.307065	1875.510808	20.589159
62.496551	1876.678816	20.594176
62.470657	1874.922138	20.599194
62.418817	1898.280924	20.604211
62.404953	1909.882881	20.609229
63.034034	1905.588138	20.614247
62.946036	1897.108265	20.619264
62.983405	1911.007390	20.624282
62.867252	1912.484535	20.629299
62.622540	1904.718860	20.634317
63.154307	1921.526101	20.639335
63.175466	1934.940384	20.644352
63.239641	1936.138944	20.649370
63.366549	1940.876727	20.654387
63.377468	1938.378218	20.659405
64.054370	1924.166681	20.664423
63.491249	1932.223424	20.669440
63.235266	1927.974348	20.674458
63.409748	1932.892433	20.679475
63.440066	1937.215123	20.684493
63.842727	1937.472617	20.689511
64.101719	1951.380623	20.694528
64.182064	1950.414360	20.699546
64.131637	1950.573516	20.704563
64.380699	1953.364764	20.709581
64.250430	1955.012534	20.714599
64.171795	1956.753729	20.719616
64.598692	1945.657738	20.724634
64.472613	1958.185650	20.729651
64.285580	1954.431611	20.734669
64.483816	1947.449904	20.739687
64.012472	1951.886003	20.744704
64.028377	1949.650614	20.749722
64.319170	1949.991940	20.754739
64.172469	1963.774498	20.759757
64.853308	1966.253877	20.764775
64.690870	1975.165587	20.769792
64.942351	1980.834066	20.774810
64.758932	1976.706632	20.779827
64.737344	1978.635624	20.784845
65.004618	1977.124159	20.789863
65.542041	1977.876649	20.794880
65.088059	1978.655577	20.799898
65.414354	1982.797891	20.804915
65.073951	1997.813926	20.809933
65.445879	1996.467428	20.814951
65.185138	2001.814107	20.819968
65.692493	2006.647293	20.824986
65.148475	1996.760208	20.830003
65.425695	2003.471373	20.835021
65.911652	2008.024663	20.840039
65.776228	2002.006823	20.845056
66.034053	2003.488905	20.850074
66.058668	2012.782279	20.855091
66.120395	2029.977316	20.860109
66.165586	2024.687610	20.865127
66.111005	2030.820614	20.870144
65.933037	2016.997865	20.875162
66.711276	2018.199289	20.880179
66.886338	2020.490827	20.885197
66.857122	2033.977490	20.890215
66.794344	2023.974452	20.895232
66.987218	2011.242860	20.900250
67.226444	1996.398738	20.905267
66.586324	1992.366842	20.910285
66.276248	1986.156634	20.915303
66.534889	2004.908689	20.920320
66.731561	2007.957986	20.925338
66.994066	2016.389704	20.930355
66.441578	2018.850671	20.935373
66.673357	2006.515563	20.940391
66.831360	2018.063614	20.945408
67.200348	2039.840250	20.950426
67.789946	2047.376098	20.955443
67.184270	2045.392998	20.960461
67.288957	2039.134505	20.965479
68.043000	2048.930134	20.970496
67.916357	2043.803053	20.975514
67.855780	2032.218717	20.980531
68.196264	2045.341773	20.985549
67.886728	2032.725070	20.990567
67.729398	2023.523200	20.995584
67.874367	2033.442691	21.000602
67.806467	2039.336784	21.005619
67.749214	2045.530072	21.010637
68.308407	2035.644698	21.015655
68.272067	2035.516519	21.020672
68.052632	2034.106140	21.025690
68.107412	2026.891241	21.030707
67.958258	2036.090129	21.035725
68.047275	2036.185106	21.040743
67.917960	2045.476971	21.045760
67.991052	2056.140558	21.050778
68.255440	2070.018255	21.055795
68.595262	2070.584135	21.060813
68.394456	2062.803448	21.065831
68.388354	2065.198346	21.070848
68.217571	2085.311673	21.075866
68.713624	2081.758473	21.080883
68.787399	2099.365725	21.085901
69.301505	2084.255254	21.090919
68.924323	2089.100786	21.095936
69.081515	2086.883956	21.100954
69.495956	2096.594016	21.105971
69.434161	2127.215641	21.110989
69.646155	2122.689595	21.116007
69.911240	2115.573550	21.121024
69.575873	2118.001214	21.126042
70.026035	2104.699330	21.131059
69.947886	2098.201368	21.136077
69.790804	2082.399727	21.141095
69.882687	2095.063762	21.146112
70.266780	2114.386300	21.151130
70.117143	2095.598294	21.156147
70.199292	2115.513779	21.161165
70.114173	2114.791754	21.166183
70.079345	2107.585326	21.171200
69.876876	2107.427517	21.176218
70.236889	2105.163981	21.181235
70.082569	2106.076056	21.186253
70.232633	2104.769557	21.191271
70.506127	2105.333408	21.196288
70.446886	2119.483502	21.201306
70.630509	2118.062216	21.206323
70.723551	2131.204977	21.211341
70.739608	2143.417456	21.216359
70.567626	2134.395876	21.221376
70.683501	2140.701917	21.226394
70.966175	2140.599557	21.231411
70.938766	2140.020144	21.236429
71.138025	2147.294001	21.241447
71.333248	2161.639463	21.246464
71.560366	2166.905386	21.251482
72.064735	2167.039791	21.256499
71.509643	2161.136507	21.261517
71.796294	2147.513412	21.266535
71.840514	2134.283502	21.271552
71.369166	2144.120083	21.276570
71.563676	2147.261882	21.281587
71.968270	2157.543628	21.286605
71.592011	2170.393930	21.291623
71.711316	2163.207671	21.296640
71.644151	2167.027885	21.301658
71.928232	2157.936835	21.306675
71.861114	2169.662539	21.311693
71.912844	2195.467011	21.316711
72.191560	2193.706218	21.321728
71.924372	2192.533220	21.326746
72.581242	2188.145235	21.331763
72.527082	2189.648380	21.336781
72.663632	2192.071098	21.341799
72.558658	2191.437578	21.346816
72.475852	2191.994764	21.351834
73.103552	2185.221681	21.356851
73.095163	2206.396215	21.361869
72.926315	2202.035232	21.366887
73.164926	2192.123607	21.371904
72.809815	2206.110488	21.376922
73.043958	2213.497892	21.381939
72.867075	2216.684935	21.386957
73.019972	2206.782150	21.391975
73.272232	2206.183881	21.396992
72.929663	2217.599661	21.402010
73.445384	2200.380552	21.407027
73.278189	2230.047060	21.412045
73.297382	2241.337731	21.417063
73.501487	2227.711672	21.422080
73.467299	2237.882334	21.427098
73.760911	2238.124393	21.432115
73.850933	2250.262339	21.437133
74.000631	2259.088386	21.442151
74.174317	2254.063365	21.447168
74.208571	2269.495070	21.452186
74.837609	2264.853617	21.457203
74.709522	2263.820999	21.462221
74.844273	2265.301792	21.467239
74.763108	2265.764033	21.472256
74.785555	2237.664049	21.477274
74.822509	2234.806106	21.482291
75.071638	2226.512053	21.487309
74.660543	2224.171413	21.492327
74.823559	2234.037465	21.497344
74.559159	2250.012549	21.502362
74.910063	2259.652314	21.507379
74.857453	2252.424940	21.512397
74.912986	2248.857889	21.517415
75.145185	2244.995924	21.522432
74.849658	2255.326307	21.527450
75.347416	2264.693998	21.532467
75.317273	2290.751111	21.537485
75.461040	2286.229796	21.542503
75.609237	2284.569687	21.547520
75.539211	2295.912145	21.552538
75.961441	2281.082388	21.557555
76.235683	2278.933188	21.562573
76.056221	2286.180527	21.567591
75.845891	2280.533780	21.572608
75.649471	2280.771586	21.577626
76.091370	2279.533767	21.582643
76.053840	2285.195201	21.587661
76.103148	2303.663146	21.592679
76.249479	2312.328771	21.597696
76.313923	2312.650625	21.602714
76.561615	2308.132207	21.607731
76.794571	2307.434575	21.612749
76.786533	2310.368561	21.617767
76.853623	2310.669901	21.622784
76.655798	2309.525782	21.627802
76.774848	2306.401134	21.632819
76.677404	2309.669155	21.637837
76.664704	2320.305176	21.642855
76.969565	2324.730823	21.647872
76.474574	2332.078546	21.652890
76.920377	2324.132616	21.657907
77.060340	2338.937727	21.662925
76.997161	2350.755233	21.667943
77.427744	2343.536350	21.672960
77.511982	2349.762673	21.677978
77.817168	2348.593893	21.682995
77.927075	2354.695908	21.688013
77.793512	2349.991287	21.693031
77.811900	2332.828033	21.698048
77.814219	2352.295837	21.703066
78.200398	2346.948887	21.708083
78.208713	2347.121173	21.713101
77.778929	2356.812253	21.718119
77.919998	2356.223298	21.723136
77.974004	2359.756632	21.728154
78.274808	2377.193628	21.733171
78.219653	2373.342110	21.738189
78.425306	2377.960725	21.743207
78.831127	2377.633507	21.748224
78.681908	2379.100807	21.753242
78.987411	2370.273983	21.758259
79.054224	2374.187454	21.763277
78.702531	2371.809221	21.768295
79.009304	2387.542046	21.773312
79.056072	2396.459780	21.778330
78.960856	2403.371036	21.783347
79.514740	2407.328627	21.788365
79.323017	2403.793146	21.793383
79.522187	2387.446736	21.798400
79.641222	2400.300810	21.803418
79.345135	2407.797181	21.808435
79.523846	2398.198841	21.813453
79.366162	2398.769391	21.818471
79.776948	2415.013161	21.823488
79.705546	2417.591527	21.828506
79.947070	2423.062817	21.833523
80.275795	2418.303044	21.838541
79.852283	2423.747821	21.843559
80.403810	2413.094643	21.848576
80.228362	2417.126300	21.853594
80.390601	2414.297420	21.858611
80.510009	2421.803284	21.863629
80.259461	2428.422136	21.868647
80.845392	2437.435825	21.873664
80.935155	2436.093794	21.878682
80.803085	2444.279360	21.883699
81.020152	2450.754225	21.888717
80.685962	2449.290728	21.893735
80.882007	2445.976769	21.898752
80.961751	2446.092571	21.903770
81.401489	2449.108091	21.908787
81.382522	2451.210120	21.913805
80.997504	2454.963843	21.918823
81.280937	2435.870219	21.923840
81.087813	2449.930150	21.928858
81.591860	2458.891443	21.933875
81.824810	2460.129080	21.938893
81.611069	2468.891493	21.943911
81.860996	2457.009683	21.948928
82.191022	2467.195110	21.953946
82.074304	2469.828410	21.958963
82.155696	2464.097567	21.963981
82.247784	2456.519639	21.968999
81.993355	2458.326550	21.974016
82.115121	2457.952771	21.979034
81.972947	2474.586376	21.984051
82.411938	2475.547665	21.989069
82.486884	2496.495851	21.994087
82.636524	2491.701284	21.999104
82.449868	2493.087780	22.004122
82.689374	2497.634898	22.009139
82.804970	2489.379895	22.014157
82.961348	2493.043182	22.019175
82.971275	2501.622801	22.024192
83.384048	2516.464886	22.029210
83.666551	2517.771105	22.034227
83.501558	2497.660447	22.039245
83.252162	2501.570694	22.044263
83.293763	2509.384119	22.049280
83.315649	2510.373981	22.054298
83.452575	2522.929358	22.059315
83.940410	2519.291205	22.064333
83.813337	2512.404925	22.069351
83.908487	2515.345715	22.074368
83.692044	2522.134942	22.079386
83.477734	2521.544866	22.084403
83.829456	2524.390707	22.089421
83.607173	2551.355532	22.094439
83.958150	2546.715262	22.099456
84.105228	2548.355845	22.104474
84.063415	2547.899457	22.109491
84.086481	2558.111062	22.114509
84.449736	2583.210227	22.119527
84.451857	2573.941329	22.124544
84.740992	2580.676958	22.129562
84.749464	2584.761528	22.134579
84.927932	2569.795016	22.139597
84.752350	2586.946429	22.144615
85.144950	2589.283399	22.149632
85.158415	2596.650764	22.154650
85.260686	2613.692912	22.159667
85.549391	2595.715069	22.164685
85.344395	2604.462335	22.169703
85.322245	2595.591500	22.174720
85.500867	2590.604135	22.179738
85.570620	2600.597243	22.184755
85.969750	2607.880611	22.189773
85.929069	2621.024430	22.194791
86.024900	2625.807911	22.199808
86.182494	2621.570610	22.204826
86.204366	2633.271529	22.209843
86.539291	2614.827988	22.214861
86.441563	2615.328013	22.219879
86.547345	2610.299728	22.224896
86.849749	2615.442744	22.229914
86.697643	2615.370300	22.234931
86.924310	2619.276709	22.239949
86.669521	2610.290775	22.244967
86.762500	2617.641074	22.249984
86.932801	2603.404173	22.255002
86.790010	2615.224013	22.260019
86.871644	2611.842316	22.265037
86.947505	2622.633190	22.270055
86.812681	2634.346815	22.275072
86.939921	2639.245573	22.280090
86.806974	2640.934800	22.285107
87.486367	2645.905697	22.290125
87.049167	2668.232748	22.295143
87.374763	2670.148549	22.300160
87.920505	2664.627104	22.305178
87.460313	2671.214169	22.310195
87.894129	2671.580894	22.315213
88.054961	2696.742234	22.320231
88.208815	2688.760902	22.325248
88.583160	2692.922830	22.330266
88.300779	2696.222476	22.335283
89.068900	2692.809998	22.340301
88.932761	2699.332505	22.345319
89.097337	2680.532218	22.350336
89.060401	2664.068635	22.355354
88.547143	2659.631960	22.360371
88.835388	2663.579384	22.365389
88.738569	2677.537590	22.370407
88.989441	2679.876145	22.375424
89.107234	2682.817360	22.380442
88.835643	2686.519130	22.385459
89.167291	2683.897232	22.390477
89.234852	2697.213178	22.395495
89.067332	2681.082945	22.400512
89.205607	2676.124658	22.405530
89.269721	2696.579271	22.410547
89.615931	2703.964731	22.415565
89.623179	2712.136077	22.420583
89.533556	2696.364586	22.425600
89.552406	2699.403644	22.430618
89.651081	2726.046661	22.435635
89.834331	2718.840327	22.440653
90.016332	2731.075847	22.445671
89.942826	2737.951777	22.450688
90.245810	2740.632299	22.455706
90.349192	2758.548778	22.460723
90.580633	2752.357826	22.465741
90.680319	2755.132963	22.470759
90.483956	2766.587187	22.475776
90.771273	2763.488774	22.480794
90.968755	2759.770205	22.485811
91.132525	2747.777024	22.490829
91.267606	2753.725244	22.495847
91.225488	2765.853149	22.500864
91.516379	2771.222515	22.505882
91.297976	2787.828898	22.510899
91.608900	2792.680819	22.515917
91.786560	2778.790552	22.520935
91.635461	2787.075696	22.525952
92.073113	2788.828124	22.530970
91.863679	2781.472291	22.535987
91.430322	2777.378853	22.541005
91.918642	2777.827712	22.546023
91.792374	2779.922517	22.551040
92.344539	2787.506451	22.556058
92.297813	2804.541937	22.561075
92.393306	2798.833639	22.566093
92.470210	2805.495781	22.571111
92.368628	2806.883403	22.576128
92.815028	2802.563491	22.581146
92.553431	2803.399636	22.586163
92.927004	2811.458342	22.591181
92.884976	2825.045247	22.596199
93.044435	2834.585323	22.601216
93.241376	2839.507272	22.606234
93.094348	2841.942505	22.611251
93.231888	2835.072194	22.616269
93.166819	2838.257225	22.621287
93.412100	2839.184015	22.626304
93.510763	2841.278668	22.631322
93.521953	2868.848145	22.636339
93.705529	2845.835304	22.641357
93.784684	2855.309927	22.646375
93.711161	2866.038849	22.651392
93.789172	2854.908133	22.656410
94.061536	2881.495160	22.661427
94.199155	2887.271368	22.666445
94.440502	2886.183567	22.671463
94.300999	2892.691752	22.676480
94.699498	2894.900244	22.681498
94.338226	2891.986926	22.686515
94.536506	2889.459075	22.691533
94.705578	2906.614518	22.696551
94.579244	2921.410650	22.701568
94.999827	2921.113659	22.706586
94.951353	2924.682559	22.711603
95.219307	2931.467509	22.716621
95.281187	2925.632836	22.721639
95.217715	2918.259512	22.726656
95.416040	2916.302879	22.731674
95.611113	2930.762068	22.736691
95.647351	2951.971586	22.741709
95.805851	2947.651965	22.746727
95.636060	2947.076561	22.751744
95.935135	2948.834584	22.756762
95.804741	2949.039245	22.761779
95.882087	2944.980659	22.766797
96.163719	2944.288146	22.771815
95.830231	2951.766157	22.776832
96.172079	2959.558936	22.781850
96.018267	2970.674013	22.786867
96.000668	2970.860036	22.791885
96.473571	2979.052015	22.796903
96.723269	2996.269822	22.801920
97.177769	2996.767188	22.806938
97.286064	2999.428353	22.811955
97.441629	2998.281494	22.816973
97.339328	2999.159040	22.821991
97.160118	3008.065847	22.827008
97.785973	2990.825107	22.832026
97.519159	3008.968392	22.837043
97.461820	2996.608817	22.842061
97.855669	2986.409236	22.847079
97.407622	2982.371712	22.852096
97.588364	2998.921421	22.857114
97.857224	3011.680384	22.862131
98.094574	3008.518922	22.867149
98.218530	3012.823488	22.872167
97.971793	3023.361466	22.877184
98.374426	3007.991759	22.882202
98.466114	3008.531754	22.887219
98.523071	3022.763076	22.892237
98.881180	3039.594136	22.897255
98.783011	3037.080602	22.902272
99.106622	3036.614996	22.907290
99.172885	3035.628947	22.912307
99.013080	3044.172349	22.917325
99.399776	3035.081743	22.922343
99.236979	3035.712212	22.927360
99.389280	3038.874358	22.932378
99.728451	3039.406136	22.937395
99.664680	3043.013417	22.942413
99.619181	3025.797354	22.947431
99.291943	3042.146414	22.952448
99.684668	3057.110440	22.957466
99.578540	3064.900921	22.962483
99.541413	3060.211249	22.967501
99.938126	3069.931942	22.972519
99.945521	3089.689390	22.977536
100.568041	3092.196314	22.982554
100.735416	3108.103100	22.987571
100.333700	3104.699987	22.992589
100.570755	3097.203693	22.997607
100.964160	3100.292942	23.002624
101.137900	3094.110208	23.007642
100.997066	3088.586124	23.012659
100.870562	3095.336330	23.017677
101.170407	3101.365722	23.022695
101.134302	3108.689162	23.027712
101.236022	3101.212079	23.032730
101.398101	3108.549619	23.037747
101.272015	3105.411972	23.042765
101.391285	3090.331910	23.047783
101.326955	3108.826484	23.052800
101.977376	3112.626780	23.057818
102.220070	3119.247884	23.062835
102.273613	3126.368730	23.067853
102.717343	3130.282315	23.072871
101.935454	3117.140433	23.077888
101.966240	3130.019145	23.082906
102.377255	3134.833378	23.087923
102.167282	3131.784387	23.092941
102.406901	3127.747364	23.097959
102.657301	3145.192377	23.102976
102.640457	3163.221706	23.107994
102.821686	3150.162770	23.113011
102.417605	3171.396922	23.118029
103.059057	3165.975822	23.123047
102.836565	3172.798613	23.128064
102.942314	3184.429201	23.133082
103.430265	3192.190084	23.138099
103.191203	3194.440585	23.143117
103.611756	3203.316115	23.148135
103.756575	3200.269114	23.153152
103.857329	3204.151598	23.158170
103.781222	3221.341209	23.163187
103.900227	3230.600035	23.168205
104.082881	3219.213192	23.173223
103.866774	3228.167166	23.178240
104.177441	3231.211454	23.183258
104.700970	3253.524292	23.188275
104.538578	3257.842385	23.193293
104.881694	3244.592451	23.198311
104.786192	3253.032825	23.203328
104.927341	3238.793859	23.208346
104.951410	3244.619279	23.213363
105.094469	3253.494234	23.218381
105.352758	3240.642954	23.223399
105.206979	3248.030249	23.228416
105.131582	3262.548220	23.233434
105.532856	3270.006544	23.238451
105.771893	3277.548765	23.243469
105.692332	3269.016155	23.248487
105.887902	3272.847951	23.253504
105.749296	3271.601653	23.258522
106.225157	3293.544090	23.263539
106.043045	3293.271488	23.268557
106.406959	3289.044598	23.273575
106.200684	3297.937146	23.278592
106.799824	3286.916068	23.283610
107.695308	3282.615124	23.288627
107.826666	3281.937979	23.293645
107.565553	3257.112629	23.298663
107.610961	3236.670385	23.303680
107.426691	3234.558436	23.308698
107.410347	3233.480909	23.313715
107.636782	3233.314811	23.318733
107.845686	3224.127099	23.323751
107.494029	3240.589848	23.328768
107.470549	3229.421305	23.333786
108.005013	3234.065175	23.338803
108.043709	3237.993354	23.343821
108.148933	3221.383251	23.348839
107.896022	3233.755008	23.353856
107.816006	3243.941187	23.358874
108.078857	3253.543964	23.363891
108.164681	3262.498459	23.368909
107.963140	3270.598107	23.373927
107.949366	3265.626176	23.378944
107.854226	3284.525251	23.383962
108.609264	3295.804549	23.388979
108.449695	3306.209814	23.393997
108.405075	3300.103630	23.399015
108.774299	3314.806048	23.404032
108.889587	3333.851904	23.409050
109.061555	3334.673914	23.414067
108.888196	3327.996487	23.419085
109.060281	3345.555845	23.424103
109.285525	3361.239161	23.429120
109.191941	3351.611998	23.434138
109.682797	3351.806922	23.439155
109.827245	3377.093923	23.444173
110.024865	3370.646116	23.449191
110.218161	3389.420889	23.454208
110.084151	3379.927551	23.459226
110.232792	3380.512084	23.464243
110.225275	3390.474180	23.469261
110.344237	3379.699305	23.474279
110.602740	3390.789072	23.479296
110.972999	3409.516519	23.484314
111.234570	3404.630539	23.489331
111.176390	3405.504360	23.494349
111.169653	3392.103453	23.499367
111.715951	3402.610646	23.504384
111.356754	3403.838531	23.509402
111.791985	3398.485679	23.514419
111.418159	3408.313830	23.519437
111.788263	3392.970378	23.524455
111.338981	3392.502161	23.529472
111.716566	3413.216153	23.534490
112.101715	3419.120554	23.539507
111.789686	3443.185873	23.544525
112.521221	3423.400862	23.549543
112.365428	3430.793442	23.554560
112.333197	3438.787250	23.559578
112.518703	3429.953670	23.564595
112.346908	3454.411181	23.569613
112.919934	3454.107104	23.574631
112.920238	3466.101384	23.579648
112.805981	3467.208093	23.584666
112.621700	3462.551276	23.589683
113.004111	3479.148883	23.594701
112.916242	3486.549163	23.599719
113.469363	3494.706511	23.604736
113.008963	3497.671571	23.609754
113.984894	3499.349314	23.614771
113.707510	3504.747089	23.619789
113.739494	3511.826795	23.624807
113.990329	3510.925964	23.629824
113.613139	3514.354830	23.634842
114.554341	3526.370850	23.639859
114.659988	3537.530073	23.644877
114.338239	3526.529103	23.649895
114.715104	3532.228226	23.654912
114.929493	3543.945857	23.659930
115.320972	3521.120494	23.664947
114.996789	3530.081868	23.669965
115.160383	3529.719461	23.674983
115.378544	3526.945707	23.680000
115.469952	3530.636907	23.685018
115.437937	3518.036514	23.690035
115.397830	3525.354905	23.695053
115.785392	3533.200265	23.700071
115.707031	3554.596864	23.705088
115.600864	3546.953132	23.710106
115.926793	3544.141096	23.715123
115.880738	3546.269205	23.720141
116.127027	3537.581425	23.725159
116.220247	3562.303973	23.730176
116.257951	3589.281775	23.735194
116.833349	3580.297073	23.740211
116.940608	3588.536804	23.745229
116.626906	3583.210790	23.750247
116.686068	3576.876720	23.755264
116.445493	3588.253029	23.760282
116.659836	3590.787327	23.765299
116.715168	3607.012743	23.770317
117.215483	3602.803782	23.775335
117.141859	3603.298280	23.780352
116.870549	3629.484699	23.785370
117.751322	3620.107785	23.790387
117.658774	3624.221133	23.795405
118.108950	3633.111702	23.800423
118.053552	3626.735124	23.805440
117.994773	3622.130355	23.810458
118.002513	3636.262893	23.815475
118.043262	3656.392321	23.820493
118.112679	3656.384447	23.825511
118.495978	3660.006975	23.830528
118.468058	3677.744245	23.835546
118.949938	3681.845369	23.840563
118.949151	3684.642394	23.845581
118.838715	3688.570132	23.850599
119.245296	3683.568373	23.855616
118.987116	3691.292953	23.860634
119.408878	3702.388645	23.865651
119.222880	3709.737135	23.870669
119.364834	3713.922782	23.875687
119.640801	3719.958726	23.880704
119.954399	3734.404200	23.885722
120.320340	3732.895755	23.890739
120.380965	3733.763350	23.895757
120.181388	3733.919215	23.900775
120.501690	3734.218705	23.905792
120.513247	3736.504644	23.910810
120.754162	3740.756230	23.915827
120.779091	3752.303355	23.920845
121.054834	3761.871640	23.925863
121.566471	3763.667078	23.930880
120.881051	3759.655576	23.935898
120.851337	3760.320776	23.940915
120.849216	3775.830269	23.945933
121.079100	3786.104968	23.950951
121.773247	3787.442691	23.955968
121.736270	3797.996532	23.960986
121.945889	3782.166615	23.966003
121.902606	3780.890745	23.971021
122.018926	3805.408681	23.976039
122.233381	3807.784334	23.981056
122.372673	3810.581858	23.986074
122.181445	3811.647372	23.991091
122.134847	3817.788621	23.996109
122.550403	3831.116939	24.001127
122.987114	3824.521958	24.006144
122.916331	3837.304654	24.011162
123.377854	3834.929219	24.016179
123.585844	3836.570901	24.021197
123.537004	3828.073851	24.026215
123.758207	3831.719267	24.031232
123.565253	3836.355169	24.036250
123.854703	3841.919245	24.041267
124.293196	3853.216219	24.046285
123.885778	3857.727721	24.051303
124.166797	3855.480535	24.056320
124.071010	3858.752347	24.061338
124.221400	3862.131122	24.066355
124.529550	3858.195187	24.071373
124.496380	3867.128748	24.076391
124.793938	3866.793018	24.081408
125.110057	3883.179176	24.086426
125.095781	3881.518580	24.091443
125.280503	3875.330179	24.096461
125.103871	3882.043733	24.101479
125.160521	3875.691846	24.106496
125.248556	3884.023888	24.111514
125.657978	3880.964136	24.116531
125.710876	3881.733409	24.121549
125.486319	3878.714238	24.126567
125.696135	3890.519502	24.131584
125.698811	3905.622423	24.136602
125.596865	3893.807698	24.141619
125.771668	3910.788108	24.146637
125.868667	3922.615187	24.151655
125.912427	3935.792822	24.156672
126.053918	3950.742533	24.161690
126.198436	3965.416164	24.166707
126.655071	3975.724388	24.171725
126.666790	3989.893599	24.176743
127.386331	3984.069942	24.181760
127.298026	4003.450265	24.186778
127.426144	3995.736497	24.191795
127.513146	4001.486446	24.196813
127.534576	3998.547081	24.201831
127.602744	4007.460041	24.206848
127.835150	4009.458343	24.211866
128.043030	4014.467052	24.216883
128.074396	4015.465090	24.221901
127.966304	4027.961188	24.226919
128.369193	4051.248280	24.231936
128.174350	4055.386912	24.236954
128.347859	4052.150355	24.241971
128.701097	4066.885659	24.246989
128.745905	4082.466052	24.252007
129.154012	4079.179309	24.257024
128.902803	4084.616660	24.262042
129.084881	4096.005394	24.267059
129.195292	4102.036165	24.272077
129.224427	4122.851991	24.277095
129.699065	4121.058220	24.282112
129.479579	4140.509209	24.287130
129.520151	4140.965169	24.292147
130.110933	4142.732615	24.297165
130.098773	4134.832896	24.302183
130.162488	4155.920225	24.307200
130.347604	4168.294363	24.312218
130.360056	4161.404373	24.317235
130.960128	4176.231282	24.322253
130.866938	4200.138771	24.327271
131.488179	4193.427316	24.332288
131.403987	4204.019550	24.337306
131.567744	4196.571849	24.342323
131.799491	4190.321615	24.347341
131.523151	4199.200268	24.352359
131.854753	4190.550393	24.357376
131.468354	4191.913543	24.362394
131.992044	4194.964165	24.367411
132.285342	4208.126390	24.372429
132.176187	4216.643954	24.377447
132.443706	4213.328049	24.382464
132.574919	4214.335193	24.387482
132.715480	4225.756867	24.392499
132.788438	4218.158406	24.397517
132.609363	4236.859508	24.402535
132.441862	4243.451231	24.407552
132.715488	4252.428812	24.412570
132.883406	4253.520054	24.417587
133.174358	4265.770087	24.422605
133.464595	4276.711539	24.427623
133.351189	4276.665762	24.432640
133.543516	4280.992850	24.437658
133.552276	4281.771798	24.442675
133.664216	4303.524611	24.447693
133.708052	4311.803553	24.452711
134.100211	4314.025114	24.457728
133.734260	4331.638268	24.462746
134.248752	4339.539052	24.467763
134.568295	4323.475061	24.472781
134.880134	4343.822013	24.477799
134.885351	4348.533594	24.482816
135.292899	4342.604266	24.487834
135.386465	4348.469011	24.492851
135.582331	4348.872938	24.497869
135.543530	4354.367416	24.502887
135.596588	4333.033850	24.507904
135.691068	4356.823952	24.512922
135.610087	4377.870527	24.517939
136.159182	4370.377184	24.522957
136.020297	4384.835429	24.527975
135.953119	4388.477837	24.532992
136.224972	4405.416766	24.538010
136.644286	4404.486868	24.543027
136.992344	4411.457274	24.548045
136.678549	4423.769558	24.553063
136.999727	4419.119882	24.558080
137.058704	4438.452393	24.563098
137.236428	4445.440329	24.568115
137.495769	4440.163828	24.573133
137.235879	4452.672749	24.578151
137.369587	4463.310654	24.583168
137.548275	4456.071003	24.588186
137.602041	4459.202082	24.593203
138.042659	4472.122856	24.598221
138.046028	4494.955342	24.603239
138.556753	4495.497022	24.608256
138.734935	4489.823264	24.613274
138.784357	4496.025690	24.618291
139.002856	4483.689042	24.623309
139.033893	4497.317701	24.628327
139.258777	4518.239120	24.633344
139.410724	4514.172524	24.638362
139.385495	4514.901586	24.643379
139.718196	4511.951639	24.648397
139.402767	4517.635196	24.653415
139.270319	4529.198271	24.658432
139.575062	4542.275812	24.663450
139.723442	4540.742609	24.668467
140.221075	4549.477826	24.673485
140.265477	4569.191274	24.678503
140.379005	4572.426681	24.683520
140.817656	4576.528496	24.688538
140.954441	4582.349572	24.693555
141.287218	4572.427176	24.698573
140.937563	4574.103594	24.703591
141.236742	4598.807539	24.708608
141.507195	4604.793556	24.713626
141.395811	4607.103480	24.718643
141.580437	4608.429009	24.723661
141.574869	4608.414626	24.728679
141.505317	4614.374145	24.733696
141.740235	4640.686108	24.738714
141.639107	4641.182033	24.743731
141.903770	4642.056519	24.748749
142.014551	4665.096323	24.753767
141.968319	4666.684031	24.758784
142.529653	4678.823174	24.763802
142.643585	4694.375434	24.768819
143.171906	4695.889865	24.773837
142.823975	4697.660112	24.778855
142.913534	4688.377079	24.783872
143.249089	4700.585831	24.788890
143.324195	4718.466328	24.793907
143.790324	4709.036411	24.798925
143.659853	4716.643145	24.803943
143.902572	4733.693551	24.808960
144.589907	4726.823303	24.813978
144.423973	4742.036396	24.818995
144.415210	4749.096230	24.824013
144.818386	4748.869419	24.829031
144.851253	4742.809711	24.834048
145.250094	4733.990148	24.839066
145.202192	4737.309353	24.844083
145.185964	4728.707992	24.849101
145.135715	4754.416830	24.854119
145.190771	4762.937088	24.859136
145.642178	4760.339553	24.864154
145.417891	4777.140379	24.869171
145.820995	4779.898819	24.874189
145.926804	4795.472996	24.879207
145.660605	4802.676578	24.884224
146.037640	4801.204001	24.889242
145.651673	4829.633577	24.894259
146.561581	4827.892622	24.899277
146.279374	4827.268785	24.904295
146.192359	4851.386108	24.909312
146.800759	4851.447063	24.914330
146.925803	4865.809384	24.919347
147.465818	4876.599351	24.924365
147.328301	4886.257875	24.929383
147.545252	4886.338232	24.934400
147.709037	4882.382980	24.939418
147.891104	4905.951165	24.944435
148.487963	4903.397689	24.949453
148.924348	4906.177034	24.954471
148.480060	4911.557984	24.959488
148.842503	4905.389028	24.964506
148.482275	4903.748080	24.969523
148.699627	4913.758254	24.974541
148.923864	4938.871607	24.979559
149.103938	4929.869955	24.984576
149.776030	4931.602406	24.989594
149.556584	4932.919920	24.994611
149.490706	4932.350892	24.999629
149.874978	4942.749284	25.004647
149.980546	4963.959540	25.009664
150.443670	4957.832988	25.014682
149.879404	4965.435135	25.019699
150.143338	4967.433865	25.024717
150.377844	4973.640943	25.029735
150.528318	4979.322100	25.034752
150.566916	4992.353437	25.039770
150.038323	5014.215439	25.044787
150.423436	5013.126185	25.049805
150.732157	5023.081171	25.054823
151.163579	5044.401882	25.059840
151.614088	5047.340350	25.064858
151.451006	5055.348339	25.069875
151.643192	5061.676233	25.074893
152.081098	5067.908406	25.079911
151.975910	5080.292257	25.084928
152.429485	5081.780494	25.089946
152.311356	5087.755306	25.094963
152.529976	5079.889424	25.099981
152.575933	5091.506908	25.104999
152.722077	5116.361379	25.110016
153.055377	5116.694978	25.115034
153.037909	5124.335211	25.120051
152.869805	5115.211045	25.125069
153.315011	5125.232529	25.130087
152.986896	5150.258338	25.135104
153.490384	5150.022823	25.140122
153.379023	5166.810526	25.145139
153.725188	5176.702331	25.150157
153.864088	5179.017840	25.155175
154.174818	5196.152799	25.160192
154.295337	5206.846153	25.165210
154.314967	5205.841687	25.170227
154.429271	5222.759107	25.175245
154.732885	5244.932392	25.180263
155.184378	5241.445704	25.185280
155.531083	5229.776329	25.190298
155.538667	5240.957308	25.195315
155.767908	5246.693666	25.200333
155.866117	5257.034012	25.205351
156.008117	5251.781746	25.210368
156.279897	5254.676550	25.215386
156.417406	5247.290961	25.220403
156.312776	5246.374747	25.225421
156.373215	5268.453193	25.230439
156.509673	5284.367709	25.235456
156.974174	5275.703941	25.240474
156.901685	5281.794132	25.245491
157.140849	5310.168145	25.250509
157.432759	5318.958264	25.255527
157.186170	5313.342188	25.260544
157.594254	5313.067706	25.265562
157.423734	5329.942137	25.270579
157.594541	5342.176645	25.275597
158.031364	5349.436777	25.280615
157.952544	5367.354080	25.285632
158.435395	5370.317979	25.290650
158.083046	5373.148195	25.295667
158.377794	5390.730150	25.300685
159.221670	5378.208751	25.305703
159.336883	5395.030923	25.310720
159.480363	5401.586711	25.315738
159.355881	5401.856178	25.320755
159.672814	5417.112596	25.325773
159.996201	5416.205581	25.330791
160.102830	5430.551383	25.335808
160.151316	5424.774688	25.340826
160.114497	5420.072834	25.345843
160.202086	5439.166792	25.350861
160.894070	5444.507438	25.355879
160.563639	5459.611383	25.360896
161.118343	5458.268464	25.365914
161.179696	5452.948345	25.370931
160.929265	5458.890821	25.375949
161.028525	5472.432278	25.380967
160.917332	5491.991477	25.385984
161.241386	5490.715408	25.391002
161.600309	5513.386686	25.396019
161.729602	5525.797114	25.401037
161.763945	5522.932503	25.406055
161.843974	5550.608360	25.411072
162.406792	5553.898491	25.416090
162.527510	5563.021399	25.421107
162.181941	5575.519384	25.426125
162.460017	5591.555318	25.431143
162.225147	5594.829604	25.436160
162.984055	5604.450705	25.441178
163.109790	5610.443697	25.446195
163.494754	5624.150703	25.451213
163.843046	5637.717305	25.456231
163.771205	5641.703730	25.461248
163.936512	5642.967966	25.466266
164.085353	5653.857364	25.471283
164.104880	5665.142197	25.476301
164.254477	5680.313909	25.481319
164.428750	5674.059195	25.486336
164.656861	5684.878029	25.491354
164.890466	5702.058969	25.496371
165.206192	5703.677539	25.501389
165.206404	5701.927336	25.506407
165.266970	5719.508586	25.511424
165.821031	5727.784301	25.516442
165.871286	5722.042249	25.521459
165.787933	5727.986752	25.526477
166.406102	5728.998982	25.531495
166.474045	5739.714381	25.536512
166.975065	5752.219888	25.541530
166.800751	5751.523846	25.546547
166.938624	5752.378791	25.551565
167.166016	5740.987840	25.556583
167.008239	5754.184559	25.561600
167.424753	5763.201223	25.566618
167.694272	5771.465307	25.571635
167.255738	5778.428877	25.576653
167.958251	5790.048649	25.581671
167.559496	5817.189043	25.586688
167.826098	5809.921249	25.591706
168.005337	5827.913385	25.596723
167.916630	5838.297599	25.601741
168.352030	5842.965722	25.606759
168.494596	5869.594267	25.611776
168.237721	5877.144091	25.616794
168.931498	5885.884668	25.621811
169.063325	5902.288047	25.626829
169.329733	5898.509706	25.631847
169.210388	5936.317832	25.636864
169.759521	5938.831852	25.641882
169.878928	5941.170777	25.646899
169.477479	5958.179721	25.651917
169.959709	5961.815193	25.656935
170.199324	5977.563742	25.661952
170.633045	5997.716311	25.666970
170.605367	6012.523877	25.671988
171.106593	6022.660718	25.677005
170.932041	6025.991671	25.682023
171.474665	6028.318958	25.687040
171.951020	6032.883507	25.692058
172.502913	6042.402452	25.697076
172.745201	6039.421093	25.702093
172.868250	6037.042987	25.707111
172.805985	6038.488185	25.712128
173.314021	6038.636615	25.717146
173.258864	6028.991604	25.722164
172.982249	6027.969488	25.727181
173.079815	6022.060430	25.732199
173.233756	6035.611058	25.737216
173.325654	6043.078922	25.742234
173.307346	6036.984249	25.747252
173.068225	6059.286165	25.752269
173.828429	6053.770834	25.757287
173.800241	6069.351094	25.762304
173.659813	6088.177960	25.767322
173.898973	6103.984988	25.772340
173.705215	6124.917877	25.777357
173.974699	6126.866623	25.782375
174.128184	6149.888958	25.787392
174.368870	6170.409128	25.792410
174.825078	6184.282442	25.797428
174.744357	6202.196287	25.802445
175.278910	6204.160311	25.807463
175.040552	6215.085723	25.812480
175.356912	6225.988792	25.817498
175.452759	6230.507591	25.822516
175.689616	6249.010852	25.827533
176.245695	6266.572271	25.832551
176.215039	6283.018644	25.837568
176.177787	6292.217693	25.842586
177.021264	6294.165337	25.847604
176.616661	6317.364394	25.852621
177.048559	6325.298348	25.857639
177.057701	6327.738241	25.862656
177.012054	6354.125826	25.867674
177.497774	6358.095123	25.872692
177.453385	6368.051428	25.877709
178.224729	6390.064789	25.882727
178.117258	6397.264136	25.887744
178.254986	6405.696418	25.892762
178.660632	6411.748605	25.897780
178.442518	6429.507427	25.902797
178.632565	6430.184863	25.907815
179.120427	6442.410373	25.912832
179.288540	6450.621086	25.917850
179.251646	6461.670890	25.922868
179.628300	6486.590253	25.927885
179.891525	6483.350189	25.932903
180.378384	6487.523305	25.937920
180.673721	6494.375778	25.942938
181.042339	6493.803025	25.947956
180.791805	6514.543415	25.952973
181.244214	6501.155333	25.957991
181.394026	6496.071471	25.963008
181.266659	6519.364413	25.968026
181.712698	6526.484966	25.973044
181.509844	6539.316101	25.978061
181.458161	6546.911883	25.983079
181.477104	6563.555116	25.988096
181.861734	6564.105903	25.993114
182.276966	6573.208303	25.998132
182.318323	6596.758573	26.003149
182.209855	6606.741367	26.008167
182.717324	6613.539941	26.013184
182.552672	6640.643860	26.018202
182.887813	6638.756703	26.023220
183.119963	6658.662273	26.028237
183.477190	6669.130471	26.033255
183.417388	6683.918775	26.038272
183.242859	6700.764231	26.043290
184.139907	6703.333120	26.048308
184.256076	6733.423659	26.053325
184.062428	6727.352177	26.058343
184.528783	6732.757328	26.063360
184.516472	6747.427588	26.068378
184.772329	6762.066941	26.073396
184.609084	6779.533571	26.078413
184.926687	6779.321275	26.083431
185.456712	6796.815926	26.088448
185.633397	6815.995282	26.093466
185.816062	6810.628672	26.098484
186.020078	6835.332182	26.103501
186.383614	6854.449998	26.108519
186.448236	6854.086547	26.113536
186.091623	6861.691910	26.118554
187.000549	6887.476124	26.123572
186.914990	6891.959718	26.128589
187.152511	6874.520176	26.133607
187.306096	6901.883049	26.138624
187.264034	6918.526498	26.143642
187.828566	6902.267792	26.148660
187.568002	6934.040185	26.153677
187.778559	6935.108037	26.158695
188.519426	6927.702303	26.163712
189.001064	6949.561128	26.168730
189.151884	6943.119984	26.173748
189.387931	6957.135106	26.178765
189.484846	6963.720506	26.183783
189.872124	6948.952758	26.188800
189.843063	6946.375980	26.193818
189.863315	6946.510511	26.198836
189.885070	6963.685307	26.203853
190.199755	6971.901216	26.208871
190.259224	6969.131031	26.213888
190.453182	6990.563330	26.218906
190.588389	6998.200907	26.223924
190.515143	7011.483551	26.228941
190.471327	7020.726638	26.233959
190.899486	7030.389491	26.238976
190.981274	7055.107241	26.243994
191.295179	7068.499232	26.249012
191.591571	7072.666961	26.254029
191.538738	7083.437096	26.259047
191.878953	7105.979489	26.264064
192.029155	7105.587717	26.269082
192.845671	7121.366532	26.274100
192.807226	7144.343277	26.279117
192.974567	7151.029744	26.284135
192.944282	7144.241194	26.289152
193.214766	7160.048048	26.294170
193.498391	7161.213316	26.299188
193.491512	7172.921008	26.304205
193.814668	7192.898851	26.309223
194.034268	7192.249887	26.314240
194.494978	7202.099637	26.319258
194.757992	7202.725674	26.324276
194.873727	7213.529478	26.329293
194.965155	7221.409882	26.334311
195.298356	7212.123696	26.339328
195.280961	7237.370044	26.344346
195.596635	7248.891399	26.349364
195.979956	7248.921053	26.354381
195.660335	7245.628283	26.359399
196.126808	7271.658713	26.364416
196.096249	7282.206357	26.369434
196.425899	7280.058557	26.374452
196.448837	7306.459244	26.379469
196.498003	7320.580387	26.384487
196.875478	7324.041714	26.389504
196.782759	7349.582641	26.394522
197.200644	7354.562847	26.399540
197.562148	7370.251701	26.404557
197.526618	7381.305074	26.409575
197.970528	7396.029722	26.414592
197.880297	7400.717430	26.419610
198.355675	7416.297730	26.424628
198.628151	7444.108153	26.429645
198.759836	7445.916803	26.434663
198.970461	7447.860478	26.439680
199.123527	7465.490616	26.444698
199.349384	7469.422014	26.449716
199.696659	7469.955381	26.454733
199.784127	7487.353017	26.459751
199.975557	7500.819956	26.464768
200.139281	7506.453375	26.469786
200.004365	7493.747463	26.474804
200.291716	7517.065505	26.479821
200.730728	7530.120606	26.484839
201.012703	7527.259216	26.489856
200.867934	7555.345910	26.494874
201.266564	7561.256362	26.499892
201.521858	7568.486878	26.504909
201.532799	7586.564360	26.509927
201.871962	7591.732495	26.514944
202.199640	7596.741860	26.519962
202.413547	7620.860572	26.524980
202.233556	7637.332244	26.529997
202.521142	7644.812642	26.535015
202.710427	7641.417590	26.540032
203.170501	7647.159616	26.545050
203.422652	7642.232537	26.550068
203.905432	7662.908406	26.555085
203.911377	7676.421105	26.560103
204.008126	7672.733384	26.565120
204.312798	7694.565776	26.570138
204.073570	7699.084440	26.575156
204.554082	7699.888002	26.580173
204.339317	7728.330750	26.585191
204.790918	7739.572461	26.590208
205.085998	7753.427318	26.595226
205.296155	7759.126403	26.600244
205.341210	7767.664514	26.605261
205.757822	7791.370371	26.610279
206.027459	7792.367876	26.615296
206.113841	7811.096314	26.620314
206.333104	7828.544222	26.625332
206.786618	7830.030382	26.630349
206.880730	7842.955279	26.635367
207.117342	7847.052756	26.640384
207.442373	7863.272674	26.645402
207.648484	7860.097689	26.650420
207.745985	7879.543457	26.655437
207.648826	7889.770926	26.660455
207.747697	7901.073394	26.665472
208.236838	7927.298853	26.670490
208.499183	7922.746483	26.675508
208.857825	7942.490219	26.680525
209.163486	7947.350537	26.685543
209.251572	7943.701202	26.690560
209.178749	7980.123099	26.695578
209.136305	7992.868263	26.700596
209.512611	7991.119070	26.705613
209.426622	8011.245099	26.710631
210.021789	8039.691633	26.715648
210.078090	8052.268519	26.720666
210.609900	8054.888538	26.725684
211.091763	8077.783824	26.730701
211.204236	8075.028317	26.735719
211.569293	8062.868650	26.740736
211.640664	8095.882591	26.745754
211.913724	8104.640766	26.750772
212.612695	8100.521858	26.755789
212.528456	8112.405278	26.760807
212.692618	8105.420363	26.765824
212.628996	8122.949203	26.770842
212.923559	8119.885572	26.775860
213.022953	8130.721058	26.780877
213.150638	8142.120541	26.785895
213.677757	8153.140564	26.790912
213.720711	8157.522158	26.795930
213.478982	8177.783610	26.800948
213.782504	8188.453089	26.805965
213.784915	8194.067724	26.810983
214.035135	8197.680230	26.816000
214.486666	8232.859052	26.821018
214.198309	8238.346103	26.826036
214.516329	8252.436259	26.831053
214.715128	8265.622237	26.836071
214.949345	8283.584074	26.841088
214.861632	8306.318605	26.846106
215.241867	8337.436600	26.851124
215.626231	8349.047441	26.856141
215.619063	8369.336544	26.861159
215.953145	8386.080068	26.866176
216.037738	8411.839154	26.871194
216.478209	8437.119674	26.876212
216.607050	8441.183916	26.881229
216.683719	8470.965298	26.886247
217.058975	8494.944478	26.891264
217.747335	8496.717199	26.896282
217.592576	8507.346827	26.901300
218.183040	8521.727746	26.906317
218.209816	8542.161901	26.911335
218.690107	8563.003190	26.916352
218.706026	8577.212074	26.921370
218.810238	8590.971603	26.926388
219.385797	8590.579621	26.931405
219.377458	8605.616415	26.936423
219.928562	8613.538925	26.941440
220.258217	8629.977832	26.946458
220.463323	8638.089058	26.951476
220.711573	8631.609079	26.956493
220.901441	8645.724698	26.961511
221.526080	8653.051432	26.966528
221.552532	8666.631688	26.971546
221.603908	8658.735740	26.976564
221.978740	8664.532393	26.981581
221.922013	8686.460522	26.986599
222.142020	8690.839004	26.991616
222.144172	8706.109667	26.996634
222.118926	8713.072000	27.001652
222.424664	8726.155627	27.006669
222.623613	8751.423780	27.011687
222.883863	8761.096538	27.016704
223.652735	8782.552068	27.021722
223.667399	8795.790177	27.026740
223.789924	8806.238715	27.031757
223.726192	8821.853554	27.036775
223.942690	8826.123956	27.041792
224.113467	8847.613802	27.046810
224.078696	8870.126937	27.051828
224.759129	8871.178730	27.056845
224.718106	8903.323654	27.061863
225.502276	8920.135160	27.066880
225.699297	8948.651474	27.071898
225.866389	8945.707205	27.076916
226.176515	8950.556857	27.081933
225.966601	8983.267033	27.086951
226.183149	8982.357001	27.091968
226.518195	8994.639679	27.096986
226.631480	9025.479399	27.102004
227.103532	9030.259002	27.107021
227.284812	9048.136719	27.112039
227.578819	9070.545407	27.117056
227.681676	9075.029994	27.122074
227.920790	9094.703547	27.127092
228.699321	9093.416310	27.132109
228.578645	9111.952858	27.137127
228.748564	9130.279942	27.142144
228.913772	9129.077493	27.147162
228.999267	9145.817208	27.152180
229.460916	9148.326130	27.157197
229.436454	9160.486381	27.162215
229.683045	9172.827134	27.167232
229.756899	9183.572252	27.172250
230.009237	9192.634557	27.177268
230.844083	9197.854445	27.182285
231.184042	9224.743932	27.187303
231.255762	9228.185310	27.192320
231.899690	9233.332779	27.197338
231.869943	9253.181703	27.202356
232.053119	9242.965245	27.207373
232.331295	9245.779396	27.212391
232.210292	9255.387054	27.217408
232.550856	9281.683417	27.222426
232.243746	9282.959838	27.227444
232.849151	9300.333756	27.232461
233.026612	9325.604798	27.237479
232.977023	9331.122877	27.242496
233.555243	9336.194591	27.247514
233.671418	9346.694946	27.252532
233.615722	9371.526459	27.257549
234.177699	9378.535422	27.262567
234.555893	9385.989075	27.267584
234.845434	9400.176330	27.272602
234.854290	9419.022661	27.277620
235.205102	9425.648272	27.282637
235.382115	9446.172194	27.287655
235.632179	9463.964186	27.292672
235.783864	9474.000324	27.297690
235.793717	9499.161487	27.302708
236.057301	9512.277147	27.307725
236.208921	9529.599471	27.312743
236.560965	9548.415249	27.317760
237.086185	9564.662914	27.322778
237.151764	9576.292668	27.327796
238.013806	9592.581599	27.332813
238.077163	9607.420024	27.337831
238.486610	9621.509685	27.342848
238.563445	9618.162726	27.347866
238.703627	9638.286530	27.352884
238.987973	9649.335895	27.357901
239.062918	9654.601928	27.362919
239.159566	9653.654166	27.367936
239.344355	9679.011205	27.372954
239.844342	9695.337217	27.377972
240.019812	9706.229740	27.382989
239.940710	9719.733811	27.388007
239.838981	9741.808675	27.393024
240.349430	9750.270963	27.398042
240.510041	9784.317374	27.403060
240.955672	9800.922657	27.408077
240.889528	9818.426999	27.413095
241.213309	9844.789294	27.418112
241.889803	9856.387638	27.423130
241.865594	9882.375825	27.428148
242.130110	9898.887463	27.433165
242.363357	9920.615779	27.438183
242.334328	9929.153902	27.443200
243.196914	9953.124090	27.448218
243.023721	9967.856204	27.453236
243.685227	9987.003414	27.458253
243.602184	9985.395284	27.463271
244.085164	10019.525211	27.468288
244.494746	10026.406036	27.473306
244.654077	10042.916297	27.478324
244.911728	10053.705681	27.483341
245.060035	10060.569034	27.488359
245.052295	10069.748855	27.493376
245.067602	10082.495603	27.498394
245.380831	10106.493768	27.503412
245.878566	10119.074192	27.508429
246.067057	10130.211410	27.513447
246.059545	10163.639687	27.518464
246.479981	10171.330137	27.523482
246.362459	10184.112303	27.528500
246.741144	10208.271530	27.533517
247.160883	10215.585584	27.538535
247.045611	10242.844249	27.543552
247.701567	10255.253698	27.548570
247.721061	10282.260148	27.553588
248.364811	10296.718954	27.558605
248.786527	10306.633019	27.563623
248.802237	10328.990992	27.568640
248.992341	10334.654933	27.573658
249.523205	10348.160375	27.578676
249.985042	10368.836937	27.583693
250.158575	10381.404962	27.588711
250.426205	10393.536801	27.593728
250.524673	10405.971517	27.598746
250.672292	10423.627110	27.603764
250.754628	10434.152678	27.608781
251.486207	10444.276376	27.613799
251.114314	10466.040030	27.618816
251.418781	10479.377389	27.623834
251.631227	10504.535023	27.628852
251.967897	10511.562022	27.633869
252.203858	10533.992601	27.638887
252.085561	10555.129975	27.643904
252.570839	10583.740234	27.648922
252.994407	10613.222532	27.653940
253.098654	10620.576293	27.658957
253.363694	10636.003096	27.663975
253.740706	10659.048621	27.668992
254.168132	10683.650319	27.674010
254.266046	10694.051383	27.679028
254.646312	10713.449173	27.684045
255.375122	10731.629044	27.689063
255.366200	10742.759918	27.694080
255.596164	10749.369813	27.699098
255.673794	10780.924643	27.704116
255.907324	10780.693902	27.709133
256.339126	10807.935617	27.714151
256.503651	10819.309664	27.719168
256.890139	10832.321816	27.724186
257.406186	10834.458083	27.729204
257.279476	10864.504412	27.734221
258.073813	10869.343979	27.739239
258.051886	10877.020415	27.744256
258.393137	10902.201510	27.749274
258.716886	10910.618852	27.754292
258.481936	10912.850057	27.759309
259.077291	10936.973802	27.764327
258.792048	10955.034719	27.769344
259.228070	10969.984572	27.774362
259.047362	10995.280406	27.779380
259.242355	11021.665134	27.784397
259.805976	11030.309174	27.789415
259.864281	11054.892863	27.794432
260.402075	11087.179732	27.799450
260.686104	11107.872448	27.804468
261.012863	11119.721714	27.809485
261.336581	11142.250511	27.814503
261.199491	11164.382019	27.819520
261.508353	11174.122266	27.824538
262.323169	11210.092931	27.829556
262.058283	11211.676846	27.834573
262.509282	11222.634384	27.839591
262.574566	11251.180516	27.844608
263.016251	11267.947112	27.849626
263.094660	11281.717953	27.854644
263.541578	11301.739606	27.859661
263.998008	11316.454016	27.864679
263.819494	11348.639965	27.869696
264.123352	11346.165027	27.874714
264.696339	11374.343899	27.879732
264.825972	11397.710233	27.884749
265.320237	11416.436181	27.889767
265.287870	11440.888126	27.894784
265.779342	11453.625834	27.899802
266.219088	11469.192375	27.904820
266.043631	11503.131742	27.909837
266.705364	11504.668947	27.914855
266.864742	11523.537792	27.919872
266.918959	11526.848634	27.924890
267.361582	11558.184771	27.929908
267.255264	11571.378992	27.934925
267.783983	11586.468514	27.939943
267.857454	11619.384622	27.944960
268.122016	11634.453232	27.949978
268.263022	11652.889614	27.954996
268.623550	11693.938138	27.960013
269.266631	11712.412173	27.965031
269.393606	11726.713438	27.970048
269.603170	11750.206520	27.975066
270.025139	11778.668664	27.980084
270.180223	11786.159517	27.985101
270.459830	11805.112820	27.990119
270.525333	11827.901886	27.995136
270.914279	11845.068551	28.000154
271.274280	11878.458591	28.005172
271.274578	11901.813938	28.010189
271.806654	11918.864862	28.015207
272.106506	11952.031800	28.020224
272.427688	11969.012840	28.025242
273.239454	11979.340132	28.030260
273.278814	11999.415810	28.035277
273.868667	12013.749576	28.040295
274.348833	12029.761402	28.045312
274.268160	12041.150040	28.050330
275.031263	12065.165840	28.055348
274.666351	12066.212526	28.060365
275.100908	12075.781296	28.065383
275.207399	12096.848106	28.070400
275.539354	12105.981637	28.075418
275.633754	12123.484816	28.080436
275.698520	12149.631357	28.085453
276.504994	12142.285679	28.090471
276.938289	12156.328735	28.095488
277.442092	12177.112573	28.100506
277.376932	12182.883944	28.105524
277.529383	12195.174835	28.110541
278.102474	12211.608732	28.115559
277.894261	12238.456773	28.120576
278.319999	12245.428068	28.125594
278.663565	12251.993030	28.130612
278.761392	12285.711635	28.135629
278.773534	12288.246485	28.140647
279.136164	12316.563395	28.145664
279.141740	12330.964037	28.150682
279.311302	12348.639395	28.155700
279.443346	12379.552596	28.160717
280.119779	12397.393222	28.165735
279.807867	12427.696022	28.170752
280.510874	12451.438709	28.175770
280.823044	12462.772197	28.180788
280.828160	12493.203945	28.185805
281.033912	12517.705634	28.190823
281.433255	12541.838969	28.195840
281.709497	12568.316808	28.200858
282.045167	12591.808406	28.205876
282.248197	12620.756493	28.210893
282.847627	12631.970948	28.215911
283.100473	12651.091177	28.220928
283.280423	12680.667158	28.225946
283.730203	12704.743558	28.230964
284.444467	12712.415845	28.235981
285.084629	12725.342720	28.240999
285.233647	12739.171686	28.246016
285.629426	12749.551659	28.251034
285.685318	12769.982460	28.256052
285.862488	12782.848786	28.261069
285.914943	12788.359860	28.266087
286.259386	12816.144126	28.271104
286.084580	12846.833167	28.276122
286.763299	12854.224616	28.281140
286.901866	12873.666526	28.286157
287.233611	12899.448729	28.291175
287.188967	12931.156397	28.296192
287.560726	12950.783626	28.301210
287.807242	12968.803850	28.306228
288.117600	12992.648448	28.311245
288.444887	13013.846218	28.316263
288.774479	13042.096590	28.321280
289.143109	13068.545805	28.326298
289.457202	13087.374377	28.331316
289.873881	13127.445838	28.336333
290.165160	13131.642803	28.341351
290.662250	13141.572964	28.346368
291.090878	13175.684710	28.351386
291.321242	13180.008356	28.356404
291.552871	13209.731190	28.361421
291.767572	13220.056293	28.366439
292.292569	13240.107645	28.371456
291.987712	13264.799611	28.376474
292.465919	13288.333281	28.381492
292.752706	13305.573534	28.386509
293.449049	13319.849907	28.391527
293.281470	13355.872648	28.396544
293.351708	13376.776149	28.401562
293.906787	13393.589263	28.406580
293.986163	13423.011459	28.411597
294.484040	13442.471904	28.416615
294.634622	13464.648070	28.421632
294.571418	13498.756660	28.426650
294.933563	13527.065532	28.431668
295.231417	13554.220576	28.436685
295.767139	13582.001347	28.441703
296.106744	13613.155226	28.446720
296.203607	13637.650601	28.451738
296.891027	13666.908180	28.456756
296.822605	13693.107585	28.461773
297.332059	13705.103490	28.466791
297.795215	13746.035491	28.471808
297.472297	13763.570782	28.476826
298.283707	13792.040691	28.481844
298.589859	13815.260028	28.486861
299.272044	13842.240179	28.491879
299.181522	13861.825125	28.496896
299.522179	13896.668340	28.501914
299.892954	13900.095984	28.506932
300.031777	13926.359227	28.511949
300.507847	13955.084951	28.516967
300.910681	13955.792179	28.521984
301.179212	13976.113733	28.527002
301.270243	13987.723563	28.532020
301.588566	14023.024576	28.537037
301.686355	14049.477592	28.542055
302.282055	14065.493631	28.547072
302.425334	14081.333872	28.552090
302.707526	14088.948986	28.557108
302.806389	14130.230517	28.562125
303.311529	14155.021665	28.567143
303.728643	14174.519972	28.572160
303.296153	14203.255986	28.577178
304.180958	14230.636667	28.582196
304.328447	14257.992649	28.587213
304.705206	14290.073015	28.592231
305.000211	14308.154482	28.597248
305.152578	14356.079414	28.602266
305.925095	14376.917033	28.607284
305.701538	14400.125439	28.612301
306.047709	14428.712725	28.617319
306.308113	14449.858815	28.622336
306.741527	14479.500213	28.627354
307.038791	14519.886380	28.632372
307.445057	14544.494323	28.637389
307.588645	14559.873249	28.642407
308.239099	14594.569077	28.647424
308.283252	14633.917866	28.652442
308.937968	14656.250333	28.657460
309.679617	14678.193407	28.662477
309.892830	14690.809457	28.667495
310.174822	14699.546923	28.672512
309.837345	14739.745383	28.677530
310.688120	14762.505767	28.682548
311.418824	14780.753741	28.687565
312.073864	14790.791202	28.692583
312.174655	14813.346195	28.697600
312.250896	14836.830330	28.702618
312.416706	14829.251272	28.707636
312.505122	14866.721141	28.712653
313.118890	14888.175033	28.717671
313.138887	14908.050281	28.722688
313.275348	14929.122916	28.727706
313.756562	14943.245583	28.732724
313.984954	14963.864971	28.737741
314.337489	14994.660057	28.742759
314.817070	15020.049294	28.747776
314.601302	15041.664071	28.752794
315.183103	15070.185191	28.757812
315.683378	15110.395877	28.762829
315.325856	15123.593511	28.767847
315.955969	15156.724275	28.772864
315.752994	15199.216690	28.777882
316.349138	15223.266353	28.782900
316.874368	15250.435523	28.787917
317.005118	15290.871599	28.792935
317.565336	15310.407515	28.797952
317.650667	15346.964946	28.802970
318.219238	15371.742745	28.807988
318.262539	15405.519390	28.813005
318.307413	15440.588132	28.818023
319.204312	15471.817406	28.823040
319.454861	15499.141111	28.828058
319.615270	15528.514328	28.833076
320.066888	15564.501121	28.838093
320.268589	15596.978608	28.843111
321.199622	15625.556476	28.848128
321.305571	15639.667673	28.853146
321.654034	15653.809737	28.858164
322.072978	15682.592079	28.863181
322.302023	15699.045390	28.868199
322.496835	15704.098963	28.873216
322.711867	15741.625569	28.878234
323.015357	15760.484211	28.883252
323.241456	15788.433379	28.888269
323.390845	15818.212391	28.893287
323.862378	15835.546162	28.898304
323.915763	15880.090918	28.903322
324.777083	15900.726706	28.908340
325.437987	15925.127612	28.913357
325.609004	15940.036810	28.918375
326.137955	15963.851234	28.923392
326.544248	15976.828809	28.928410
327.024039	15986.935366	28.933428
326.975980	16012.465325	28.938445
327.198940	16033.996324	28.943463
327.406225	16050.037515	28.948480
327.592369	16090.601954	28.953498
328.363147	16103.052913	28.958516
328.238401	16140.278808	28.963533
328.114218	16167.864116	28.968551
328.491506	16190.443102	28.973568
328.899324	16223.007559	28.978586
329.683929	16254.463346	28.983604
329.963810	16271.403712	28.988621
329.971661	16312.562376	28.993639
330.402932	16336.921456	28.998656
330.610020	16365.732120	29.003674
331.166609	16405.856313	29.008692
331.901867	16426.932824	29.013709
332.375577	16446.118748	29.018727
332.423657	16482.089119	29.023744
332.654815	16507.668285	29.028762
333.128427	16525.727435	29.033780
333.625901	16557.965686	29.038797
333.418150	16589.289755	29.043815
334.207802	16609.296821	29.048832
334.252111	16639.318487	29.053850
334.364811	16678.047775	29.058868
334.917353	16700.037428	29.063885
335.182571	16732.657977	29.068903
335.636538	16757.803552	29.073920
335.825441	16780.940886	29.078938
336.162522	16807.103511	29.083956
336.760539	16840.575549	29.088973
336.857864	16868.566746	29.093991
337.340600	16905.897335	29.099008
337.526217	16934.655805	29.104026
337.836012	16957.106724	29.109044
338.340627	16994.047754	29.114061
338.547206	17028.757466	29.119079
338.815190	17054.000416	29.124096
339.142191	17090.811817	29.129114
339.532522	17129.622394	29.134132
340.015146	17148.917999	29.139149
340.187108	17180.634387	29.144167
341.066342	17202.063231	29.149184
340.524298	17230.143330	29.154202
341.156988	17269.429594	29.159220
341.566069	17303.966158	29.164237
341.754692	17342.399187	29.169255
342.254739	17352.884671	29.174272
342.705237	17399.615525	29.179290
343.365131	17428.696850	29.184308
343.658211	17434.784442	29.189325
343.484314	17470.724294	29.194343
343.748681	17507.852749	29.199360
343.911508	17528.648543	29.204378
344.798370	17552.612628	29.209396
345.060292	17570.599146	29.214413
345.111621	17617.316176	29.219431
345.641478	17644.171747	29.224448
345.988829	17679.255195	29.229466
346.447010	17692.469867	29.234484
346.831916	17718.113783	29.239501
347.269518	17757.398766	29.244519
347.693041	17771.676846	29.249536
347.832779	17800.296245	29.254554
347.965891	17835.919798	29.259572
348.862366	17855.579742	29.264589
348.864719	17883.022499	29.269607
349.527842	17905.332805	29.274624
349.906870	17937.018019	29.279642
350.019580	17953.538520	29.284660
350.351582	17980.892306	29.289677
350.550934	18019.865779	29.294695
351.258704	18037.340967	29.299712
351.423960	18077.639496	29.304730
351.471172	18114.460000	29.309748
351.682558	18140.796826	29.314765
351.765538	18175.838311	29.319783
352.482458	18215.573176	29.324800
352.755562	18245.239996	29.329818
353.568788	18262.272421	29.334836
353.751735	18301.819864	29.339853
354.000309	18355.712941	29.344871
354.479778	18371.545929	29.349888
354.920149	18413.859975	29.354906
354.509451	18449.491145	29.359924
355.548191	18470.190715	29.364941
356.091317	18515.506566	29.369959
356.345913	18542.224652	29.374976
356.708635	18573.392039	29.379994
356.994900	18597.352834	29.385012
357.422516	18634.553006	29.390029
357.969721	18661.074777	29.395047
358.465523	18688.293913	29.400064
358.875481	18723.329830	29.405082
358.925479	18744.267167	29.410100
359.638260	18776.419027	29.415117
359.830517	18793.401686	29.420135
359.652171	18825.352494	29.425152
360.392429	18864.940048	29.430170
360.787513	18892.474077	29.435188
361.269320	18916.141366	29.440205
361.455008	18949.473007	29.445223
362.161950	18988.571404	29.450240
362.425887	19000.510888	29.455258
362.551797	19030.606965	29.460276
363.146908	19059.682955	29.465293
363.105302	19085.013258	29.470311
363.566660	19131.204967	29.475328
364.192445	19156.161883	29.480346
364.295763	19183.892769	29.485364
365.107848	19213.768635	29.490381
365.390258	19235.922951	29.495399
365.938604	19255.802865	29.500416
366.156066	19287.347113	29.505434
366.417893	19314.959029	29.510452
366.924770	19333.909548	29.515469
366.992254	19368.951387	29.520487
367.441794	19399.344617	29.525504
367.610950	19427.050845	29.530522
367.704891	19458.765576	29.535540
367.781923	19485.095208	29.540557
367.964854	19525.332859	29.545575
368.560186	19549.149392	29.550592
369.175468	19592.447997	29.555610
369.249627	19637.514929	29.560628
369.554859	19650.032889	29.565645
369.811888	19700.107836	29.570663
370.328371	19743.516161	29.575680
370.688110	19778.293043	29.580698
370.948489	19808.431370	29.585716
371.564174	19844.419329	29.590733
371.934368	19894.526611	29.595751
372.575225	19912.199279	29.600768
373.059518	19949.894330	29.605786
372.892277	19989.134768	29.610804
373.430272	20017.064799	29.615821
373.900608	20053.056728	29.620839
374.462296	20097.677067	29.625856
374.845579	20133.076635	29.630874
374.976437	20166.880085	29.635892
375.863130	20184.167199	29.640909
376.144256	20213.410582	29.645927
376.655654	20245.855517	29.650944
377.415848	20269.742013	29.655962
378.095226	20298.607626	29.660980
378.687939	20320.376350	29.665997
378.456705	20334.299762	29.671015
378.800894	20353.987714	29.676032
379.565561	20386.614938	29.681050
379.597611	20405.988782	29.686068
380.397257	20423.183329	29.691085
380.472332	20457.601935	29.696103
380.409166	20478.675229	29.701120
381.306300	20517.427370	29.706138
380.990437	20549.766782	29.711156
381.451628	20574.395170	29.716173
381.380608	20616.157693	29.721191
381.769881	20647.622537	29.726208
382.288237	20693.526983	29.731226
382.688401	20740.141573	29.736244
383.507383	20767.859342	29.741261
383.527491	20811.883720	29.746279
383.692873	20847.253011	29.751296
384.222522	20883.410348	29.756314
384.374738	20920.028962	29.761332
385.073903	20961.155913	29.766349
385.225932	21002.056474	29.771367
385.666388	21034.304989	29.776384
386.180734	21080.392458	29.781402
386.389555	21114.843924	29.786420
387.217903	21148.381220	29.791437
387.845844	21184.117810	29.796455
388.483115	21220.265980	29.801472
388.796641	21241.691054	29.806490
389.341835	21277.818300	29.811508
389.468411	21296.070846	29.816525
389.727633	21327.851687	29.821543
390.051576	21366.583825	29.826560
390.644418	21388.224649	29.831578
390.533885	21429.112871	29.836596
391.148539	21460.865204	29.841613
391.367006	21509.484194	29.846631
391.417720	21534.949580	29.851648
391.820598	21583.082701	29.856666
392.111279	21614.355970	29.861684
392.446689	21651.707394	29.866701
393.160712	21699.147794	29.871719
393.420504	21743.339975	29.876736
393.841067	21763.406382	29.881754
393.798676	21807.661263	29.886772
394.383263	21844.708669	29.891789
394.713366	21891.386910	29.896807
395.008949	21925.951836	29.901824
395.606615	21974.678227	29.906842
395.695031	22021.827162	29.911860
396.132957	22062.270015	29.916877
396.679896	22104.262091	29.921895
396.990721	22144.991006	29.926912
397.846319	22178.404469	29.931930
398.275323	22225.500866	29.936948
398.544240	22263.394374	29.941965
398.815657	22300.059374	29.946983
399.515466	22348.938675	29.952000
400.257402	22375.716413	29.957018
400.301223	22416.747082	29.962036
400.958910	22451.931221	29.967053
401.416469	22487.266741	29.972071
401.454887	22520.659790	29.977088
401.957946	22558.192074	29.982106
402.272570	22607.406937	29.987124
402.830755	22636.868931	29.992141
403.159165	22673.033416	29.997159
403.487897	22724.374763	30.002176
404.056220	22753.828980	30.007194
404.090472	22797.052128	30.012212
404.669943	22829.760436	30.017229
405.179065	22868.192684	30.022247
405.619983	22919.008405	30.027264
406.239365	22959.032426	30.032282
406.079023	23005.520432	30.037300
407.111329	23035.030938	30.042317
407.368819	23065.804699	30.047335
407.657068	23129.901455	30.052352
408.002753	23157.811738	30.057370
408.547376	23198.421015	30.062388
408.938091	23242.991256	30.067405
409.276252	23290.616487	30.072423
409.354608	23331.761928	30.077440
409.970053	23368.820208	30.082458
409.825317	23417.235085	30.087476
410.778210	23458.561175	30.092493
411.053812	23513.537000	30.097511
411.679898	23549.990034	30.102528
412.470082	23589.276232	30.107546
412.592876	23635.511068	30.112564
413.191539	23677.394458	30.117581
413.397892	23716.443124	30.122599
413.632389	23756.652447	30.127616
414.257024	23796.759578	30.132634
414.481889	23838.455986	30.137652
414.918994	23886.457586	30.142669
415.498073	23925.255952	30.147687
416.061065	23974.522069	30.152704
416.547350	24008.766484	30.157722
416.945483	24052.199203	30.162740
417.177713	24088.817796	30.167757
417.796160	24128.248720	30.172775
418.224751	24160.390084	30.177792
418.520032	24206.512839	30.182810
418.519433	24250.111269	30.187828
418.879663	24290.231709	30.192845
419.322631	24347.435836	30.197863
419.685098	24389.604408	30.202880
420.413898	24437.706028	30.207898
420.955989	24478.541127	30.212916
421.360554	24512.405855	30.217933
422.040774	24541.401622	30.222951
422.367744	24580.448121	30.227968
423.175190	24601.335447	30.232986
423.343872	24634.332708	30.238004
423.736151	24667.797685	30.243021
424.220330	24697.594020	30.248039
423.902177	24741.279278	30.253056
424.544267	24779.301271	30.258074
424.732933	24820.231841	30.263092
424.900833	24863.051852	30.268109
425.494475	24906.858136	30.273127
425.750307	24960.015916	30.278144
426.184812	24999.696857	30.283162
426.915223	25051.319508	30.288180
427.548702	25103.046632	30.293197
428.007590	25140.003768	30.298215
428.382763	25190.291563	30.303232
429.077033	25227.621574	30.308250
429.547748	25269.049080	30.313268
430.426359	25294.239872	30.318285
430.927263	25321.908892	30.323303
431.083419	25361.748616	30.328320
431.899693	25391.708923	30.333338
432.377692	25432.985820	30.338356
432.541969	25469.635958	30.343373
432.788075	25504.773017	30.348391
433.088312	25544.870059	30.353408
433.595226	25579.114233	30.358426
433.781972	25620.094349	30.363444
434.065388	25659.139478	30.368461
434.733378	25706.906235	30.373479
434.931489	25758.328802	30.378496
435.137183	25804.019682	30.383514
435.606414	25856.996776	30.388532
435.872270	25898.511690	30.393549
436.623347	25931.361643	30.398567
436.810859	25990.214089	30.403584
437.725598	26024.519524	30.408602
438.544413	26066.350362	30.413620
439.041536	26115.936339	30.418637
439.680419	26143.241699	30.423655
439.893282	26183.356250	30.428672
440.600497	26224.493118	30.433690
440.722021	26266.455397	30.438708
441.018318	26305.831042	30.443725
441.467681	26347.528050	30.448743
441.528256	26387.983632	30.453760
442.128783	26447.037513	30.458778
442.248404	26486.130511	30.463796
442.620767	26536.252416	30.468813
443.234729	26576.875663	30.473831
443.371096	26619.858256	30.478848
443.726960	26682.990516	30.483866
444.367419	26731.602081	30.488884
444.557856	26785.719401	30.493901
445.004154	26849.184280	30.498919
445.590664	26897.518206	30.503936
446.145640	26953.181263	30.508954
446.772270	27001.653944	30.513972
446.832794	27056.582100	30.518989
447.613550	27097.308347	30.524007
448.515866	27152.451021	30.529024
448.631143	27189.499312	30.534042
449.465844	27233.251244	30.539060
449.581882	27278.900935	30.544077
450.322246	27313.370236	30.549095
450.554658	27352.351950	30.554112
451.199193	27397.227050	30.559130
451.617762	27440.694981	30.564148
452.045228	27479.159020	30.569165
452.086896	27511.652909	30.574183
452.947565	27548.386443	30.579200
453.418224	27598.643459	30.584218
453.376354	27635.226612	30.589236
453.680491	27685.467229	30.594253
454.496576	27725.643451	30.599271
454.370829	27785.856491	30.604288
455.212905	27824.394755	30.609306
456.140282	27863.379538	30.614324
455.950640	27920.140231	30.619341
456.696765	27954.881135	30.624359
456.789614	28016.487755	30.629376
457.807830	28061.447960	30.634394
458.291633	28104.285396	30.639412
458.487655	28162.762205	30.644429
459.170275	28197.476237	30.649447
459.337339	28246.261756	30.654464
459.661587	28306.026913	30.659482
460.485712	28340.784101	30.664500
460.839985	28392.478955	30.669517
461.318398	28443.658223	30.674535
461.826046	28486.044749	30.679552
462.124434	28533.348915	30.684570
463.020912	28587.229094	30.689588
463.495617	28633.961858	30.694605
464.159777	28670.932129	30.699623
464.687711	28720.974764	30.704640
465.461810	28769.683571	30.709658
465.604298	28796.068890	30.714676
465.940842	28836.904174	30.719693
466.292890	28885.913296	30.724711
466.657443	28929.248796	30.729728
467.155966	28978.290765	30.734746
467.671634	29022.787613	30.739764
467.998447	29065.580812	30.744781
469.156156	29106.388345	30.749799
469.716542	29153.023187	30.754816
469.738754	29192.138408	30.759834
470.395689	29235.618804	30.764852
470.398149	29287.229334	30.769869
471.026505	29333.875517	30.774887
470.998559	29380.062418	30.779904
471.458163	29428.285603	30.784922
472.214936	29483.623810	30.789940
472.083380	29541.269799	30.794957
473.113838	29589.897560	30.799975
473.618093	29651.716485	30.804992
473.697627	29691.299702	30.810010
474.602564	29738.380785	30.815028
475.163001	29796.162528	30.820045
475.552123	29832.051362	30.825063
476.117831	29890.170091	30.830080
476.648390	29944.294749	30.835098
477.931636	29988.500092	30.840116
477.726503	30027.919735	30.845133
478.316045	30084.801711	30.850151
478.658773	30138.380696	30.855168
478.828743	30169.845729	30.860186
479.061726	30216.345072	30.865204
480.385380	30283.479029	30.870221
480.505406	30326.647041	30.875239
481.256805	30377.720676	30.880256
481.232029	30425.982471	30.885274
481.878450	30467.874556	30.890292
482.203581	30518.220867	30.895309
482.516025	30554.685399	30.900327
483.124887	30616.708149	30.905344
483.157038	30663.639356	30.910362
484.223593	30706.144046	30.915380
484.281458	30757.939066	30.920397
484.992132	30801.654267	30.925415
485.768487	30858.930654	30.930432
485.750986	30904.485753	30.935450
486.431362	30944.537279	30.940468
486.530140	30996.237913	30.945485
487.239355	31045.698895	30.950503
487.587471	31102.021495	30.955520
487.676450	31158.014807	30.960538
488.530622	31218.478537	30.965556
489.094528	31280.839177	30.970573
489.700602	31330.652418	30.975591
490.303557	31383.914611	30.980608
490.602342	31437.741457	30.985626
491.462811	31473.975416	30.990644
491.744939	31530.972826	30.995661
492.447018	31586.162690	31.000679
493.039208	31627.441840	31.005696
493.154005	31688.467858	31.010714
493.950139	31737.430578	31.015732
493.827630	31794.782781	31.020749
494.498547	31841.223573	31.025767
495.619473	31904.147506	31.030784
496.111809	31945.112624	31.035802
496.814376	31995.274642	31.040820
497.017040	32058.486467	31.045837
498.000805	32098.455819	31.050855
498.082978	32147.818410	31.055872
498.657064	32198.967671	31.060890
499.446136	32237.079631	31.065908
499.853041	32285.303636	31.070925
500.441995	32328.011054	31.075943
501.054255	32375.715509	31.080960
501.322937	32422.883689	31.085978
501.654804	32470.445410	31.090996
501.999518	32520.137981	31.096013
502.441358	32563.586477	31.101031
503.003041	32624.434655	31.106048
503.178068	32694.345324	31.111066
503.466551	32746.067101	31.116084
503.967438	32825.459285	31.121101
504.670376	32877.191868	31.126119
504.943660	32937.710145	31.131136
505.141225	32996.830770	31.136154
505.765253	33065.763211	31.141172
506.143434	33135.301310	31.146189
506.713369	33200.942870	31.151207
507.479538	33267.419949	31.156224
507.963751	33328.267575	31.161242
508.301300	33411.712304	31.166260
508.836576	33471.816816	31.171277
509.274994	33534.395490	31.176295
510.048854	33601.875935	31.181312
510.368633	33666.184837	31.186330
511.316343	33719.958803	31.191348
512.311473	33776.915127	31.196365
512.642310	33836.953678	31.201383
513.481729	33874.549704	31.206400
513.870795	33930.025804	31.211418
514.543933	33988.108810	31.216436
514.882585	34040.791627	31.221453
515.152811	34105.334339	31.226471
515.852133	34151.426284	31.231488
516.170349	34201.806368	31.236506
516.672370	34244.832547	31.241524
517.223636	34296.430257	31.246541
517.496990	34350.961230	31.251559
518.360933	34397.509403	31.256576
518.695717	34455.747647	31.261594
519.108188	34502.976512	31.266612
519.653630	34546.614719	31.271629
520.174203	34605.699984	31.276647
520.985155	34656.735198	31.281664
521.488719	34707.846573	31.286682
522.079229	34755.359096	31.291700
522.437971	34809.782708	31.296717
522.763484	34855.846716	31.301735
523.137037	34910.867738	31.306752
523.431178	34977.432355	31.311770
524.359985	35024.293325	31.316788
524.656131	35104.300690	31.321805
524.846441	35175.256794	31.326823
525.428790	35219.316559	31.331840
526.018785	35292.428638	31.336858
526.445501	35353.138081	31.341876
527.128714	35410.116458	31.346893
527.638921	35472.150494	31.351911
528.276037	35534.349966	31.356928
529.030120	35599.465082	31.361946
530.025404	35655.717394	31.366964
530.575839	35711.207108	31.371981
531.052509	35768.558402	31.376999
531.719786	35824.597191	31.382016
531.699021	35885.981935	31.387034
532.339711	35942.792319	31.392052
532.796297	35992.507695	31.397069
533.182583	36054.671517	31.402087
533.983786	36108.262325	31.407104
534.821999	36171.854038	31.412122
535.298605	36219.884729	31.417140
535.889152	36288.538564	31.422157
536.217841	36350.473088	31.427175
537.052000	36405.668790	31.432192
537.466998	36464.982777	31.437210
537.718437	36524.778411	31.442228
538.050487	36581.307284	31.447245
538.585491	36657.179587	31.452263
539.990562	36693.545740	31.457280
540.347218	36745.116407	31.462298
541.004985	36794.185392	31.467316
541.355428	36852.615061	31.472333
541.900811	36907.500238	31.477351
542.983331	36950.254025	31.482368
543.472042	37009.100034	31.487386
544.230890	37054.946654	31.492404
544.703760	37092.682610	31.497421
544.802514	37156.011775	31.502439
545.033087	37195.924522	31.507456
545.689528	37267.351587	31.512474
546.349798	37315.702031	31.517492
546.601454	37372.473901	31.522509
546.962677	37442.908959	31.527527
547.290272	37496.298106	31.532544
547.666710	37566.081001	31.537562
547.994025	37628.537739	31.542580
548.468474	37708.858659	31.547597
548.954114	37781.663592	31.552615
549.735282	37855.654019	31.557632
549.846423	37933.659449	31.562650
550.524744	38015.646018	31.567668
551.233886	38074.620060	31.572685
551.486331	38155.648724	31.577703
552.338378	38220.984413	31.582720
552.542333	38296.448042	31.587738
553.357985	38354.856243	31.592756
553.870809	38432.418746	31.597773
554.652186	38501.810137	31.602791
554.984210	38564.676476	31.607808
555.524397	38633.909372	31.612826
556.567201	38696.179034	31.617844
557.144862	38753.763038	31.622861
557.211358	38823.422076	31.627879
558.107131	38889.276889	31.632896
558.849315	38948.481885	31.637914
559.662528	38994.314990	31.642932
560.691900	39061.776983	31.647949
560.896707	39126.847252	31.652967
561.405110	39184.586096	31.657984
561.806039	39248.999469	31.663002
562.383777	39317.698520	31.668020
562.618635	39382.682678	31.673037
563.242829	39453.482980	31.678055
563.740004	39516.246432	31.683072
564.061397	39584.370189	31.688090
564.828228	39657.158313	31.693108
565.131792	39729.896989	31.698125
565.612428	39821.570229	31.703143
566.325691	39883.525946	31.708160
566.787080	39961.482245	31.713178
567.132810	40035.626089	31.718196
568.153647	40093.693519	31.723213
568.775667	40182.384495	31.728231
569.556366	40250.996731	31.733248
569.904101	40324.033502	31.738266
570.209682	40404.135415	31.743284
571.372494	40478.505947	31.748301
571.882635	40548.388708	31.753319
572.551750	40624.953079	31.758336
572.884524	40700.986207	31.763354
573.695330	40766.899733	31.768372
574.311966	40826.336752	31.773389
574.303335	40917.992139	31.778407
575.205354	40978.373680	31.783424
575.827689	41065.190724	31.788442
576.246331	41132.590806	31.793460
576.940223	41203.168581	31.798477
577.168253	41289.578320	31.803495
578.137446	41360.224870	31.808512
578.442467	41440.082033	31.813530
579.291463	41506.266544	31.818548
580.283418	41577.491000	31.823565
581.103557	41644.204784	31.828583
581.689124	41699.072561	31.833600
581.974824	41773.811039	31.838618
583.119897	41847.827047	31.843636
583.704354	41907.108737	31.848653
584.152908	41973.389480	31.853671
584.573488	42032.768090	31.858688
585.051422	42096.465351	31.863706
585.452074	42175.479685	31.868724
586.155009	42233.060291	31.873741
586.250855	42317.012292	31.878759
586.990091	42386.649555	31.883776
587.236104	42462.003491	31.888794
587.563509	42552.146752	31.893812
588.303134	42618.804762	31.898829
588.371702	42707.602513	31.903847
589.165640	42799.677703	31.908864
589.710665	42878.412337	31.913882
590.440767	42945.751836	31.918900
591.356113	43025.773941	31.923917
591.726762	43104.503612	31.928935
592.762337	43166.571881	31.933952
593.201227	43240.975307	31.938970
593.587073	43308.849688	31.943988
594.566472	43386.113046	31.949005
594.746442	43458.167108	31.954023
595.443346	43529.110043	31.959040
596.191427	43603.018718	31.964058
596.741269	43689.538086	31.969076
597.369863	43746.684235	31.974093
597.775930	43829.389024	31.979111
598.644190	43908.478760	31.984128
599.065304	43982.796544	31.989146
599.519367	44060.007407	31.994164
600.555564	44134.334710	31.999181
601.020580	44211.282352	32.004199
601.501186	44277.894405	32.009216
602.011775	44356.536821	32.014234
602.558500	44440.130359	32.019252
603.453396	44520.197024	32.024269
603.846107	44599.156709	32.029287
604.164353	44680.029668	32.034304
605.269480	44764.242810	32.039322
605.382266	44853.125607	32.044340
606.235115	44926.981202	32.049357
606.829593	45014.910656	32.054375
607.331072	45102.584357	32.059392
608.200123	45187.760329	32.064410
609.086484	45264.803755	32.069428
609.653065	45335.797208	32.074445
610.195571	45431.747336	32.079463
610.435017	45508.472369	32.084480
611.469668	45577.731827	32.089498
611.926601	45656.094949	32.094516
613.077195	45735.846753	32.099533
613.444067	45809.501936	32.104551
614.159575	45898.804815	32.109568
614.326771	45983.213093	32.114586
614.876431	46073.311449	32.119604
615.582297	46154.666692	32.124621
616.277493	46244.511340	32.129639
616.862507	46323.310773	32.134656
617.389831	46400.528684	32.139674
618.001715	46500.410229	32.144692
618.351784	46580.174694	32.149709
618.684068	46672.642085	32.154727
619.041567	46770.123132	32.159744
619.738464	46869.901029	32.164762
620.098730	46969.277198	32.169780
621.285420	47051.415777	32.174797
621.692883	47142.995245	32.179815
622.495499	47236.916018	32.184832
623.351659	47341.438147	32.189850
624.318930	47431.123535	32.194868
625.121981	47501.037773	32.199885
626.009159	47589.158298	32.204903
626.890690	47668.874331	32.209920
627.758493	47741.544923	32.214938
627.989776	47820.601660	32.219956
628.818304	47891.640449	32.224973
629.290617	47974.156809	32.229991
629.294862	48053.372008	32.235008
630.588651	48126.700017	32.240026
630.895175	48212.620474	32.245044
631.630291	48292.192795	32.250061
632.181901	48366.951644	32.255079
632.900235	48446.827380	32.260096
633.793657	48511.308412	32.265114
633.999542	48596.527237	32.270132
635.001424	48651.643547	32.275149
635.317279	48730.964847	32.280167
635.519416	48810.658944	32.285184
636.173576	48890.303986	32.290202
636.789775	48971.278804	32.295220
637.254830	49040.818753	32.300237
637.843481	49135.845351	32.305255
638.231853	49216.723047	32.310272
639.001843	49297.298054	32.315290
639.515036	49394.125822	32.320308
640.258169	49493.793060	32.325325
640.875328	49590.948880	32.330343
641.045626	49677.435316	32.335360
642.480628	49762.358467	32.340378
642.759161	49854.550238	32.345396
643.272120	49939.746462	32.350413
644.044653	50033.638675	32.355431
645.172775	50125.230357	32.360448
645.859585	50212.461338	32.365466
646.502765	50315.373828	32.370484
647.241240	50396.375556	32.375501
647.735032	50496.228160	32.380519
648.479577	50577.488623	32.385536
649.212532	50667.509060	32.390554
649.643173	50759.632693	32.395572
649.916685	50820.392990	32.400589
650.647209	50936.521083	32.405607
651.184439	51037.177842	32.410624
652.266261	51116.069873	32.415642
652.796927	51213.071344	32.420660
653.243118	51311.110550	32.425677
654.040615	51396.875812	32.430695
655.041355	51503.389808	32.435712
655.663900	51592.159997	32.440730
656.185864	51693.880764	32.445748
657.230292	51780.652379	32.450765
658.057492	51858.588297	32.455783
658.697948	51949.858633	32.460800
659.394677	52029.841338	32.465818
659.853193	52125.728600	32.470836
660.873158	52211.176486	32.475853
661.273293	52291.777781	32.480871
661.691672	52384.283909	32.485888
662.514777	52485.112635	32.490906
663.065585	52576.151213	32.495924
663.712761	52675.045381	32.500941
664.110112	52768.043230	32.505959
664.793690	52860.463616	32.510976
665.303343	52963.595500	32.515994
665.558341	53065.102245	32.521012
666.371056	53165.373995	32.526029
666.941418	53270.519000	32.531047
667.335551	53383.615580	32.536064
668.357450	53476.298890	32.541082
668.763998	53598.933855	32.546100
669.528814	53696.872510	32.551117
670.146514	53806.207353	32.556135
670.472014	53921.794832	32.561152
671.499024	54024.379407	32.566170
672.251747	54125.771580	32.571188
672.914213	54238.550836	32.576205
673.994849	54332.763697	32.581223
674.683955	54429.688766	32.586240
675.657379	54539.531243	32.591258
675.774587	54635.117663	32.596276
676.857778	54733.015260	32.601293
677.447464	54824.797110	32.606311
677.786778	54914.036756	32.611328
678.998705	55002.008127	32.616346
679.826687	55106.160168	32.621364
680.227445	55192.143551	32.626381
680.900130	55271.240096	32.631399
681.410519	55371.743696	32.636416
682.516706	55462.242823	32.641434
683.184557	55553.642416	32.646452
683.613765	55638.808034	32.651469
684.145597	55735.500178	32.656487
684.638100	55833.658773	32.661504
685.445272	55924.872813	32.666522
686.070752	56032.771951	32.671540
686.526638	56123.969108	32.676557
687.596318	56233.647220	32.681575
688.080999	56354.403695	32.686592
688.817412	56435.478334	32.691610
688.849928	56545.392643	32.696628
689.608014	56661.853613	32.701645
690.662498	56748.310803	32.706663
691.744802	56863.727434	32.711680
692.650187	56964.729948	32.716698
693.137107	57062.263730	32.721716
693.757492	57173.929447	32.726733
694.844019	57270.171031	32.731751
695.554529	57371.485820	32.736768
696.384696	57473.109935	32.741786
697.130211	57574.085091	32.746804
698.405698	57652.782026	32.751821
699.723212	57724.186867	32.756839
700.107585	57826.113883	32.761856
700.886202	57907.389783	32.766874
701.528799	57982.407605	32.771892
702.183399	58083.924827	32.776909
702.436250	58168.296376	32.781927
703.033148	58259.075670	32.786944
703.875056	58349.859150	32.791962
704.121392	58440.583423	32.796980
704.672813	58541.342787	32.801997
705.609387	58630.279412	32.807015
706.347400	58739.489049	32.812032
706.882209	58846.211536	32.817050
707.565488	58939.867474	32.822068
708.170503	59036.317187	32.827085
708.999005	59142.651524	32.832103
709.458059	59246.456571	32.837120
709.871846	59352.064289	32.842138
710.159534	59476.404698	32.847156
711.179253	59583.398596	32.852173
711.440873	59693.589450	32.857191
712.419279	59822.190910	32.862208
713.462812	59924.519005	32.867226
713.975606	60036.130040	32.872244
714.759843	60154.168005	32.877261
715.584315	60265.703566	32.882279
716.273180	60381.066503	32.887296
717.211829	60494.037969	32.892314
718.297727	60606.221080	32.897332
718.939637	60707.380839	32.902349
719.583790	60808.028840	32.907367
720.153304	60926.631324	32.912384
720.651714	61030.603393	32.917402
721.392120	61146.714247	32.922420
721.834494	61263.039300	32.927437
722.962544	61371.952361	32.932455
723.254058	61478.368761	32.937472
724.367854	61591.595520	32.942490
724.901125	61697.069397	32.947508
725.427871	61806.665531	32.952525
726.128192	61895.453376	32.957543
726.634770	62025.524557	32.962560
727.421133	62125.706902	32.967578
727.879376	62249.732859	32.972596
728.742135	62360.553158	32.977613
729.671887	62470.787860	32.982631
729.822080	62604.745314	32.987648
730.960217	62722.170994	32.992666
731.133867	62839.813507	32.997684
732.141414	62962.583837	33.002701
733.267270	63081.024868	33.007719
733.698540	63197.735727	33.012736
734.553217	63315.887920	33.017754
735.812240	63433.455744	33.022772
736.723250	63547.485335	33.027789
737.746949	63649.683828	33.032807
738.085370	63766.135157	33.037824
738.983169	63881.780543	33.042842
739.904924	63984.364138	33.047860
740.773311	64100.059857	33.052877
741.399348	64213.565031	33.057895
741.608248	64328.441794	33.062912
742.666455	64457.059432	33.067930
743.171334	64564.486974	33.072948
743.839154	64676.375989	33.077965
744.650010	64790.207794	33.082983
745.579132	64918.527267	33.088000
746.589589	65034.634608	33.093018
747.459079	65151.119858	33.098036
748.057462	65273.250990	33.103053
748.771769	65388.107087	33.108071
749.555170	65504.330418	33.113088
749.948736	65626.503780	33.118106
750.840478	65743.747236	33.123124
751.371856	65866.177387	33.128141
752.474722	65986.510046	33.133159
752.986592	66112.554321	33.138176
754.142052	66223.865485	33.143194
754.818504	66339.251458	33.148212
755.544718	66459.668025	33.153229
756.460792	66578.865503	33.158247
757.386408	66686.658126	33.163264
757.967523	66802.334237	33.168282
759.250119	66918.445129	33.173300
759.832020	67026.372128	33.178317
760.577591	67134.639313	33.183335
761.629948	67249.576321	33.188352
762.346452	67351.913399	33.193370
764.103978	67438.192601	33.198388
764.988972	67550.086549	33.203405
765.798745	67626.003647	33.208423
766.097742	67731.641954	33.213440
767.100524	67821.296780	33.218458
767.865735	67927.737826	33.223476
768.030179	68033.621141	33.228493
768.651077	68125.774261	33.233511
769.305668	68234.972526	33.238528
769.737883	68345.377648	33.243546
770.435460	68462.832839	33.248564
771.021398	68581.856027	33.253581
771.740638	68699.663000	33.258599
771.908796	68820.754308	33.263616
772.668866	68949.284594	33.268634
773.462061	69068.326886	33.273652
774.018132	69192.567955	33.278669
775.314643	69324.811617	33.283687
775.674645	69452.291989	33.288704
776.302457	69555.489002	33.293722
777.231040	69682.364763	33.298740
777.517736	69801.716112	33.303757
778.375480	69926.341606	33.308775
779.184715	70059.422704	33.313792
779.919066	70189.646570	33.318810
780.975545	70323.700106	33.323828
781.863274	70450.833799	33.328845
782.695756	70562.019000	33.333863
783.452551	70681.658066	33.338880
784.179647	70810.249362	33.343898
785.031949	70937.410784	33.348916
785.760660	71078.149462	33.353933
786.659192	71195.207275	33.358951
787.072308	71338.718607	33.363968
787.840313	71464.961311	33.368986
788.868565	71588.993015	33.374004
789.781800	71723.540600	33.379021
790.304633	71859.784841	33.384039
790.945777	72004.729936	33.389056
791.638690	72132.614014	33.394074
792.799576	72263.393462	33.399092
792.964904	72414.142350	33.404109
794.216417	72558.250585	33.409127
794.376958	72702.154216	33.414144
795.535711	72844.692546	33.419162
796.373338	72989.864782	33.424180
797.054765	73142.082776	33.429197
797.936348	73289.254293	33.434215
798.961633	73435.833971	33.439232
799.579658	73578.694094	33.444250
800.666058	73715.862481	33.449268
801.216676	73868.562497	33.454285
802.453555	74019.885537	33.459303
802.889536	74154.470224	33.464320
803.352141	74312.177308	33.469338
804.681889	74444.289070	33.474356
805.344661	74594.066734	33.479373
806.541744	74741.158089	33.484391
807.519932	74882.588732	33.489408
808.349204	75022.900249	33.494426
809.481472	75150.445074	33.499444
810.197070	75309.319177	33.504461
810.982176	75430.832915	33.509479
811.683851	75573.635439	33.514496
812.299895	75738.012114	33.519514
813.376815	75860.359117	33.524532
814.020563	75998.316993	33.529549
815.354906	76151.656205	33.534567
815.888593	76282.342142	33.539584
816.371072	76423.788733	33.544602
817.616373	76567.994206	33.549620
818.044999	76711.715683	33.554637
818.965070	76849.007164	33.559655
819.930214	76985.166293	33.564672
820.493582	77143.509628	33.569690
821.422434	77287.873271	33.574708
822.122820	77437.196167	33.579725
822.855706	77575.585629	33.584743
823.819877	77717.264579	33.589760
824.540201	77870.053067	33.594778
825.793634	78011.818963	33.599796
826.359812	78152.959240	33.604813
827.035912	78288.630202	33.609831
828.420297	78427.872480	33.614848
829.460768	78571.163484	33.619866
830.256769	78690.112836	33.624884
830.988422	78828.029628	33.629901
831.908775	78950.432295	33.634919
832.978872	79068.908310	33.639936
833.466105	79201.162515	33.644954
834.388537	79324.926809	33.649972
835.186942	79457.263982	33.654989
835.544413	79580.256422	33.660007
836.560922	79715.051266	33.665024
837.331654	79836.522060	33.670042
838.383295	79972.040068	33.675060
838.877624	80114.007965	33.680077
839.970149	80229.032759	33.685095
841.339576	80364.671461	33.690112
841.958892	80495.602139	33.695130
842.975633	80622.818110	33.700148
843.324889	80757.969781	33.705165
844.141797	80887.351973	33.710183
844.907753	81028.142187	33.715200
845.610588	81170.404944	33.720218
846.690801	81295.982209	33.725236
847.414095	81449.016104	33.730253
848.355052	81587.725036	33.735271
849.450978	81720.703297	33.740288
849.790949	81875.960500	33.745306
850.932778	82005.206894	33.750324
851.674111	82153.624638	33.755341
852.364718	82313.343701	33.760359
853.127755	82453.093157	33.765376
853.861274	82604.070874	33.770394
854.644052	82760.330130	33.775412
855.389922	82916.090458	33.780429
856.312769	83052.900836	33.785447
856.972024	83216.635934	33.790464
857.925665	83382.949028	33.795482
858.709669	83537.625505	33.800500
859.198627	83700.588744	33.805517
860.108943	83864.919680	33.810535
861.549818	84025.399918	33.815552
862.517172	84182.764559	33.820570
863.726847	84319.016386	33.825588
864.556342	84475.754162	33.830605
865.996587	84622.263156	33.835623
866.833201	84778.653858	33.840640
867.704046	84932.724376	33.845658
868.659931	85056.868784	33.850676
869.368810	85220.053246	33.855693
870.234487	85355.925142	33.860711
871.242565	85501.454504	33.865728
871.601598	85666.237325	33.870746
872.710946	85799.262426	33.875764
873.418182	85960.478367	33.880781
873.830034	86124.521792	33.885799
875.060794	86264.476661	33.890816
876.055908	86410.621286	33.895834
877.162485	86555.590549	33.900852
878.115034	86702.598212	33.905869
879.140541	86855.150115	33.910887
880.569070	86985.554116	33.915904
881.481446	87139.993124	33.920922
882.277665	87264.897050	33.925940
883.277173	87409.585597	33.930957
883.900348	87559.721859	33.935975
885.303378	87681.851303	33.940992
885.746281	87823.837559	33.946010
886.762772	87959.345436	33.951028
887.232316	88091.597095	33.956045
887.744317	88252.677630	33.961063
888.817848	88383.635281	33.966080
889.277141	88529.906956	33.971098
890.321869	88675.741179	33.976116
890.802233	88804.926094	33.981133
891.846009	88943.801545	33.986151
893.010867	89087.068359	33.991168
893.577668	89240.432914	33.996186
894.237198	89371.072084	34.001204
895.109478	89530.355354	34.006221
896.028555	89685.366865	34.011239
896.568456	89819.458066	34.016256
897.496011	89988.575463	34.021274
898.246396	90149.465055	34.026292
898.916255	90302.971352	34.031309
899.738954	90469.755396	34.036327
900.906473	90636.186247	34.041344
901.605572	90814.839698	34.046362
902.581004	90989.556901	34.051380
903.680345	91153.249769	34.056397
904.590951	91312.519672	34.061415
905.550731	91482.680234	34.066432
906.228286	91658.413446	34.071450
907.012465	91820.688363	34.076468
908.332998	91992.773843	34.081485
908.656095	92172.322239	34.086503
909.730807	92337.482872	34.091520
910.745422	92527.963420	34.096538
911.346189	92703.020784	34.101556
912.318476	92878.435785	34.106573
913.042202	93073.265987	34.111591
914.366459	93256.631738	34.116608
914.907612	93438.007947	34.121626
916.349400	93609.939389	34.126644
917.235442	93795.647388	34.131661
918.006153	93979.945455	34.136679
918.977518	94161.237054	34.141696
919.957861	94348.180564	34.146714
921.081981	94527.531901	34.151732
921.558322	94706.440856	34.156749
922.525640	94906.650830	34.161767
923.727835	95085.050292	34.166784
924.626678	95268.273593	34.171802
925.699559	95461.406944	34.176820
926.461031	95648.390211	34.181837
927.162953	95836.118975	34.186855
928.153245	96008.876114	34.191872
928.909665	96203.776573	34.196890
930.006825	96408.047396	34.201908
931.177328	96585.323628	34.206925
932.693397	96760.986925	34.211943
934.013891	96945.273496	34.216960
934.783059	97121.708327	34.221978
935.481278	97294.503700	34.226996
936.249364	97468.181282	34.232013
937.345688	97656.403152	34.237031
938.451261	97837.440176	34.242048
939.209350	98023.802629	34.247066
939.741953	98206.101692	34.252084
941.110965	98385.782513	34.257101
941.450712	98565.824472	34.262119
942.975649	98754.756178	34.267136
943.530039	98937.671031	34.272154
944.293625	99133.954346	34.277172
945.561183	99313.038189	34.282189
946.377943	99505.359039	34.287207
947.324738	99687.366269	34.292224
948.442690	99872.220688	34.297242
949.306530	100062.524864	34.302260
950.896659	100241.827954	34.307277
951.537157	100419.117631	34.312295
952.761805	100578.541369	34.317312
953.455709	100752.640142	34.322330
954.509058	100919.400175	34.327348
955.632404	101079.242640	34.332365
955.976269	101263.456320	34.337383
956.800026	101429.871418	34.342400
957.857418	101612.437702	34.347418
959.300550	101786.261582	34.352436
960.079325	101965.438573	34.357453
960.544350	102148.720622	34.362471
961.363817	102316.142550	34.367488
962.256097	102501.977746	34.372506
963.257637	102691.189875	34.377524
964.664505	102871.276201	34.382541
965.363196	103058.907531	34.387559
966.612087	103255.566790	34.392576
967.270113	103431.196646	34.397594
968.052951	103622.414521	34.402612
969.035007	103821.078618	34.407629
970.047559	104028.249032	34.412647
970.850245	104212.357480	34.417664
971.948959	104419.181213	34.422682
972.583815	104614.476877	34.427700
974.198753	104802.292519	34.432717
974.781764	105014.075365	34.437735
975.990912	105214.124665	34.442752
976.874624	105417.255949	34.447770
977.658716	105613.395624	34.452788
978.873612	105815.683816	34.457805
979.780484	106018.163734	34.462823
981.436460	106213.948670	34.467840
982.272257	106410.478376	34.472858
983.116795	106607.489366	34.477876
984.113146	106801.741175	34.482893
984.988950	107018.215842	34.487911
986.267127	107199.961820	34.492928
987.230675	107396.059841	34.497946
988.370457	107601.578428	34.502964
989.431164	107802.260871	34.507981
990.312491	107984.508374	34.512999
991.765358	108176.478478	34.518016
992.662523	108376.786970	34.523034
993.688505	108559.939120	34.528052
994.948115	108756.694922	34.533069
995.574581	108954.683959	34.538087
996.675796	109138.194965	34.543104
998.058802	109338.316471	34.548122
998.503990	109530.931323	34.553140
999.646816	109710.234242	34.558157
1000.606048	109911.164621	34.563175
1001.697106	110101.701001	34.568192
1002.694622	110301.044677	34.573210
1003.419711	110492.062228	34.578228
1005.122237	110695.700381	34.583245
1005.652058	110902.523018	34.588263
1007.138507	111087.085719	34.593280
1007.636719	111270.812143	34.598298
1008.896490	111473.769229	34.603316
1010.099672	111654.253117	34.608333
1011.204022	111838.719338	34.613351
1012.484599	112027.287235	34.618368
1013.873302	112207.452815	34.623386
1014.454850	112380.887103	34.628404
1015.417844	112571.778655	34.633421
1016.221547	112763.812583	34.638439
1017.227951	112953.217518	34.643456
1017.857690	113137.099463	34.648474
1018.505748	113323.639860	34.653492
1020.166091	113510.179085	34.658509
1021.122217	113682.812348	34.663527
1022.237474	113861.070386	34.668544
1023.475065	114038.853325	34.673562
1024.136344	114217.517981	34.678580
1025.214507	114400.181501	34.683597
1025.522468	114598.504859	34.688615
1026.177010	114786.029518	34.693632
1027.445160	114980.067148	34.698650
1028.287794	115189.049420	34.703668
1029.556861	115389.348084	34.708685
1030.247884	115581.407496	34.713703
1031.603605	115778.502090	34.718720
1032.548343	115983.191336	34.723738
1033.812839	116179.721037	34.728756
1034.807517	116379.299265	34.733773
1035.768046	116582.241917	34.738791
1036.972267	116778.342328	34.743808
1038.242059	116968.833361	34.748826
1039.378565	117181.620815	34.753844
1040.368000	117368.258590	34.758861
1041.793789	117580.583189	34.763879
1042.450315	117783.597326	34.768896
1043.789439	117982.179774	34.773914
1044.741198	118169.855308	34.778932
1045.975802	118367.621479	34.783949
1046.495567	118580.711284	34.788967
1047.349636	118788.273917	34.793984
1048.175558	118996.362188	34.799002
1049.041538	119216.951134	34.804020
1049.975788	119438.113352	34.809037
1051.170244	119661.869819	34.814055
1051.993807	119888.172730	34.819072
1053.049421	120104.441778	34.824090
1053.537362	120341.561232	34.829108
1054.936803	120572.259965	34.834125
1055.770667	120806.665192	34.839143
1056.486468	121044.690450	34.844160
1057.773928	121290.454211	34.849178
1058.585608	121535.145481	34.854196
1060.012163	121762.478562	34.859213
1061.154869	122008.196236	34.864231
1062.112585	122243.771041	34.869248
1063.897735	122468.199248	34.874266
1064.705622	122719.579142	34.879284
1065.854518	122957.903285	34.884301
1066.967412	123192.522336	34.889319
1067.804255	123426.783308	34.894336
1068.947248	123653.784985	34.899354
1070.278637	123905.075875	34.904372
1071.204314	124137.363556	34.909389
1071.903988	124366.243378	34.914407
1073.190451	124622.160616	34.919424
1074.277186	124861.993041	34.924442
1075.463462	125102.875492	34.929460
1076.794077	125350.135990	34.934477
1077.944806	125583.107456	34.939495
1078.750130	125810.890985	34.944512
1079.935078	126054.886259	34.949530
1081.141214	126291.035089	34.954548
1082.245883	126528.431857	34.959565
1083.464869	126761.274418	34.964583
1084.475198	126985.357574	34.969600
1086.035965	127207.513799	34.974618
1086.848254	127457.247129	34.979636
1088.228869	127682.934593	34.984653
1089.175001	127903.359606	34.989671
1090.094571	128138.594179	34.994688
1091.260998	128336.146851	34.999706
1092.117236	128565.577610	35.004724
1093.458576	128776.919431	35.009741
1094.349230	129003.673441	35.014759
1095.100117	129224.824598	35.019776
1096.354151	129462.612403	35.024794
1097.309179	129697.498131	35.029812
1098.058421	129918.679864	35.034829
1099.229383	130164.129810	35.039847
1100.226143	130414.325636	35.044864
1101.370962	130627.727887	35.049882
1102.400430	130875.032032	35.054900
1103.673597	131124.630199	35.059917
1104.693693	131363.523199	35.064935
1105.806072	131596.026895	35.069952
1106.741777	131848.411798	35.074970
1107.303458	132102.825229	35.079988
1109.040635	132347.641056	35.085005
1110.042865	132603.950577	35.090023
1111.444890	132846.594587	35.095040
1112.405002	133094.092370	35.100058
1113.493081	133342.394919	35.105076
1114.913416	133586.410598	35.110093
1116.140326	133834.656027	35.115111
1116.961905	134092.274993	35.120128
1118.408199	134324.870298	35.125146
1119.277814	134594.109988	35.130164
1120.999207	134839.213741	35.135181
1122.055582	135091.579018	35.140199
1123.064993	135324.469161	35.145216
1124.532753	135585.733158	35.150234
1125.620503	135843.030573	35.155252
1126.919608	136070.591770	35.160269
1128.182609	136314.413169	35.165287
1128.823006	136562.357985	35.170304
1130.447409	136815.847244	35.175322
1131.406470	137063.616470	35.180340
1132.746171	137300.966834	35.185357
1133.551550	137555.509807	35.190375
1134.284471	137812.412161	35.195392
1135.503285	138050.941585	35.200410
1137.038231	138322.295492	35.205428
1138.115980	138569.764814	35.210445
1139.226664	138811.106805	35.215463
1140.256587	139070.683068	35.220480
1141.669872	139314.628583	35.225498
1142.801399	139569.399384	35.230516
1143.717503	139821.443674	35.235533
1144.898066	140084.971425	35.240551
1145.850528	140332.778747	35.245568
1147.578207	140579.280758	35.250586
1148.550829	140851.014217	35.255604
1149.462815	141094.180489	35.260621
1150.562963	141348.652903	35.265639
1151.861355	141624.218691	35.270656
1153.194496	141872.126561	35.275674
1153.902278	142132.438840	35.280692
1155.178993	142386.851798	35.285709
1156.358418	142632.901239	35.290727
1157.617086	142904.654523	35.295744
1158.936143	143153.829290	35.300762
1160.061377	143416.263347	35.305780
1161.319266	143659.213163	35.310797
1162.433874	143932.076117	35.315815
1163.588576	144188.132877	35.320832
1164.886404	144428.038135	35.325850
1165.431485	144688.256986	35.330868
1166.532092	144947.612539	35.335885
1168.085100	145191.792378	35.340903
1168.861297	145434.986209	35.345920
1170.333494	145684.470772	35.350938
1171.428318	145937.709606	35.355956
1172.608923	146176.961348	35.360973
1173.728212	146428.094556	35.365991
1174.474139	146681.624547	35.371008
1175.728962	146939.054336	35.376026
1176.657038	147198.442154	35.381044
1177.687104	147455.265991	35.386061
1179.053992	147711.287842	35.391079
1180.398313	147987.225802	35.396096
1181.523693	148245.130182	35.401114
1182.509266	148516.413702	35.406132
1183.681305	148782.684379	35.411149
1184.953209	149061.026720	35.416167
1185.554323	149333.191457	35.421184
1186.902252	149603.357947	35.426202
1188.124301	149893.509543	35.431220
1189.189975	150172.820209	35.436237
1190.322280	150462.674043	35.441255
1191.590965	150761.411004	35.446272
1192.987191	151034.154640	35.451290
1193.756372	151330.936685	35.456308
1194.955794	151630.567204	35.461325
1196.111783	151919.553369	35.466343
1196.933648	152221.445147	35.471360
1198.195201	152521.123274	35.476378
1199.699401	152816.489382	35.481396
1200.725133	153125.774641	35.486413
1202.046568	153424.663675	35.491431
1202.837758	153735.096107	35.496448
1204.215493	154049.125288	35.501466
1204.943952	154358.634538	35.506484
1206.440464	154674.919703	35.511501
1207.953688	154982.135461	35.516519
1209.180094	155309.277427	35.521536
1210.693077	155615.699158	35.526554
1211.943177	155923.447846	35.531572
1213.518794	156223.864238	35.536589
1214.818823	156531.837822	35.541607
1215.643237	156845.638585	35.546624
1217.652744	157144.087705	35.551642
1218.903646	157446.863064	35.556660
1219.856137	157744.273435	35.561677
1221.931374	158025.327021	35.566695
1223.295036	158332.048347	35.571712
1224.775625	158602.865610	35.576730
1225.917858	158908.904858	35.581748
1227.116773	159193.511059	35.586765
1228.768746	159474.543242	35.591783
1229.042870	159775.975246	35.596800
1230.789168	160051.591732	35.601818
1231.903580	160347.358252	35.606836
1233.036040	160633.951913	35.611853
1234.672504	160912.878075	35.616871
1235.653079	161208.888613	35.621888
1236.884479	161497.514496	35.626906
1238.293005	161780.556513	35.631924
1239.395472	162063.904724	35.636941
1241.212841	162351.868988	35.641959
1241.916299	162633.866062	35.646976
1243.254343	162912.855036	35.651994
1244.565948	163202.596021	35.657012
1245.602668	163496.571083	35.662029
1246.842145	163768.515407	35.667047
1248.082237	164054.290356	35.672064
1249.247310	164342.579006	35.677082
1250.257222	164598.644126	35.682100
1251.163885	164889.986043	35.687117
1252.345014	165171.426496	35.692135
1253.244880	165458.586563	35.697152
1254.327263	165740.491129	35.702170
1255.734397	166040.055999	35.707188
1256.169427	166334.543337	35.712205
1257.767275	166631.809726	35.717223
1258.794942	166942.152070	35.722240
1260.225560	167246.986940	35.727258
1261.364194	167553.559659	35.732276
1262.456377	167876.205522	35.737293
1264.182655	168181.657898	35.742311
1265.306093	168498.047813	35.747328
1266.605506	168820.526818	35.752346
1267.987888	169130.102841	35.757364
1268.831247	169439.681162	35.762381
1270.466039	169753.800480	35.767399
1271.748945	170078.664117	35.772416
1272.685145	170399.780633	35.777434
1273.829196	170741.586374	35.782452
1275.518919	171061.733056	35.787469
1276.742506	171368.254543	35.792487
1278.093590	171688.360010	35.797504
1279.811125	172018.723736	35.802522
1281.640145	172331.255361	35.807540
1282.712200	172641.376121	35.812557
1283.767634	172960.257583	35.817575
1285.103646	173288.155422	35.822592
1286.456594	173608.375407	35.827610
1288.034085	173919.411074	35.832628
1289.154569	174254.851017	35.837645
1290.063547	174572.156000	35.842663
1291.611895	174908.925885	35.847680
1292.820607	175238.609575	35.852698
1294.275351	175561.643248	35.857716
1295.273785	175890.071719	35.862733
1296.885451	176219.048443	35.867751
1298.245764	176542.434250	35.872768
1299.672612	176868.920463	35.877786
1301.472718	177186.590607	35.882804
1302.801919	177509.480351	35.887821
1304.444316	177826.025808	35.892839
1305.674876	178145.128722	35.897856
1306.603701	178463.128603	35.902874
1307.882030	178774.270347	35.907892
1308.695315	179105.504969	35.912909
1310.405712	179431.263343	35.917927
1311.510046	179759.230643	35.922944
1312.370565	180092.164639	35.927962
1313.956043	180426.034584	35.932980
1315.774599	180740.145333	35.937997
1317.609022	181063.126961	35.943015
1319.291881	181391.504306	35.948032
1320.084127	181709.953326	35.953050
1321.750517	182021.647493	35.958068
1322.513517	182337.363723	35.963085
1323.859139	182664.065990	35.968103
1325.032459	182986.521443	35.973120
1326.068486	183322.747345	35.978138
1327.482874	183653.480589	35.983156
1328.494598	183994.080970	35.988173
1329.656415	184308.182032	35.993191
1330.797343	184663.234911	35.998208
1331.958044	185002.294016	36.003226
1333.154178	185335.637636	36.008244
1334.208850	185689.619932	36.013261
1335.935624	186012.471957	36.018279
1337.319625	186352.543476	36.023296
1338.450714	186674.368035	36.028314
1340.061008	187001.408455	36.033332
1342.006325	187315.765702	36.038349
1343.398196	187646.780897	36.043367
1344.542717	187978.321226	36.048384
1345.846499	188292.332889	36.053402
1347.272062	188616.138337	36.058420
1348.254434	188945.527825	36.063437
1349.591960	189273.070794	36.068455
1350.814985	189609.570971	36.073472
1351.853667	189952.463175	36.078490
1353.293646	190280.172700	36.083508
1354.667522	190643.857148	36.088525
1356.288491	190988.880843	36.093543
1357.340240	191344.968281	36.098560
1358.702929	191706.769749	36.103578
1359.962344	192053.636556	36.108596
1360.639352	192409.627225	36.113613
1362.392274	192773.528837	36.118631
1363.538529	193144.108555	36.123648
1365.030762	193518.721124	36.128666
1366.501380	193869.498901	36.133684
1367.751053	194252.026733	36.138701
1369.294981	194620.074324	36.143719
1370.566702	194987.331166	36.148736
1371.826792	195368.772435	36.153754
1373.328339	195733.837600	36.158772
1374.430746	196104.620107	36.163789
1375.598232	196490.361742	36.168807
1376.875678	196877.306322	36.173824
1377.988075	197268.304925	36.178842
1379.938614	197663.331701	36.183860
1380.964238	198052.305403	36.188877
1382.527680	198449.165527	36.193895
1383.890899	198832.197387	36.198912
1385.131995	199227.617314	36.203930
1386.729586	199634.013463	36.208948
1387.809364	200034.073397	36.213965
1389.264419	200435.114851	36.218983
1390.691797	200841.279769	36.224000
1392.116723	201246.076328	36.229018
1393.747354	201643.959969	36.234036
1394.947583	202056.327238	36.239053
1396.358212	202453.502750	36.244071
1397.945794	202863.004960	36.249088
1399.256869	203274.497748	36.254106
1400.830166	203682.293024	36.259124
1402.177330	204080.973641	36.264141
1403.648321	204485.540015	36.269159
1404.911459	204900.782873	36.274176
1405.878557	205314.566014	36.279194
1407.707800	205725.314296	36.284212
1409.023847	206142.739299	36.289229
1410.267180	206555.696555	36.294247
1412.046172	206970.281794	36.299264
1413.344177	207386.154910	36.304282
1415.312159	207799.646905	36.309300
1416.612022	208210.902359	36.314317
1418.335689	208611.284532	36.319335
1419.576016	209018.617863	36.324352
1420.748696	209429.100757	36.329370
1422.326459	209829.716347	36.334388
1423.712507	210247.291604	36.339405
1425.228926	210658.752577	36.344423
1426.716460	211072.798052	36.349440
1427.919461	211484.060936	36.354458
1429.442570	211874.257929	36.359476
1430.866563	212255.394025	36.364493
1432.856227	212627.168913	36.369511
1434.264222	213027.510600	36.374528
1435.259748	213404.532181	36.379546
1437.232092	213783.095777	36.384564
1438.239055	214183.331230	36.389581
1439.565025	214583.744435	36.394599
1440.933989	214966.704751	36.399616
1442.200074	215371.652020	36.404634
1443.764680	215763.827935	36.409652
1445.172855	216164.640989	36.414669
1446.339222	216581.673749	36.419687
1447.684784	216984.430895	36.424704
1448.895036	217400.418795	36.429722
1450.114123	217816.635651	36.434740
1451.459050	218241.214802	36.439757
1453.266810	218672.322884	36.444775
1454.786072	219088.648100	36.449792
1456.139901	219512.647189	36.454810
1457.764418	219990.752277	36.459828
1459.391747	220433.428592	36.464845
1460.611560	220869.037144	36.469863
1462.427647	221280.877769	36.474880
1463.456680	221724.572738	36.479898
1465.308420	222149.541985	36.484916
1466.772982	222575.694375	36.489933
1467.807226	223010.021717	36.494951
1469.365752	223446.677190	36.499968
1470.974157	223882.056217	36.504986
1472.537789	224322.016198	36.510004
1474.751234	224749.145631	36.515021
1476.385462	225174.949885	36.520039
1478.455416	225593.216372	36.525056
1480.313886	226018.377144	36.530074
1481.669451	226429.551029	36.535092
1482.870219	226845.374630	36.540109
1484.286316	227262.129326	36.545127
1485.976979	227687.425311	36.550144
1487.116731	228114.439267	36.555162
1488.677949	228525.332274	36.560180
1490.273720	228955.906043	36.565197
1491.377670	229385.902005	36.570215
1493.196607	229804.859256	36.575232
1494.586819	230242.354688	36.580250
1495.608784	230671.784151	36.585268
1496.683615	231115.506776	36.590285
1498.262174	231572.432257	36.595303
1499.619301	231996.882807	36.600320
1500.741200	232454.038899	36.605338
1502.096952	232902.445338	36.610356
1503.986662	233361.382649	36.615373
1505.176756	233824.373978	36.620391
1506.728652	234284.893910	36.625408
1507.977960	234748.614895	36.630426
1509.753039	235210.065979	36.635444
1510.858688	235673.737167	36.640461
1512.421691	236128.723121	36.645479
1514.355115	236585.884531	36.650496
1515.985452	237056.991846	36.655514
1517.659680	237510.286657	36.660532
1519.474867	237963.406967	36.665549
1521.187723	238429.296991	36.670567
1523.047129	238872.581794	36.675584
1524.318239	239336.057613	36.680602
1525.906168	239782.158151	36.685620
1527.630460	240230.345575	36.690637
1528.816461	240676.743075	36.695655
1530.948252	241107.515604	36.700672
1531.946999	241552.066141	36.705690
1533.331813	241971.761338	36.710708
1534.504873	242402.339051	36.715725
1536.150091	242841.273255	36.720743
1537.441654	243286.693456	36.725760
1539.068805	243735.005810	36.730778
1540.164595	244182.161955	36.735796
1541.638363	244630.196435	36.740813
1542.709993	245096.968934	36.745831
1544.387181	245553.074867	36.750848
1545.534782	246017.245384	36.755866
1547.119642	246493.131370	36.760884
1549.085083	246960.978895	36.765901
1550.568771	247437.010127	36.770919
1552.251179	247902.619563	36.775936
1553.691535	248379.802505	36.780954
1555.107467	248859.073200	36.785972
1557.025558	249332.037994	36.790989
1558.147550	249836.812234	36.796007
1559.773475	250305.711215	36.801024
1560.950950	250801.103872	36.806042
1562.308267	251291.158218	36.811060
1564.271110	251786.651074	36.816077
1565.591655	252310.092230	36.821095
1566.976707	252795.113797	36.826112
1568.938986	253303.767109	36.831130
1570.353907	253812.841446	36.836148
1572.132663	254314.819507	36.841165
1573.667645	254835.331716	36.846183
1575.541716	255350.072642	36.851200
1576.707006	255856.725619	36.856218
1578.466293	256370.444609	36.861236
1580.323432	256877.111032	36.866253
1581.905368	257387.404966	36.871271
1583.814927	257902.166840	36.876288
1585.335767	258416.662791	36.881306
1586.786867	258929.951041	36.886324
1588.285393	259451.741687	36.891341
1589.473575	259982.169941	36.896359
1591.267914	260491.743730	36.901376
1592.912752	261021.207588	36.906394
1594.070014	261547.830493	36.911412
1595.960246	262072.503367	36.916429
1597.406005	262614.930182	36.921447
1599.216445	263131.918803	36.926464
1600.736688	263676.212868	36.931482
1602.659553	264207.764057	36.936500
1604.782639	264730.924298	36.941517
1605.873202	265263.425201	36.946535
1608.096560	265779.175981	36.951552
1609.849783	266306.308430	36.956570
1611.410423	266826.842041	36.961588
1613.386680	267345.934902	36.966605
1614.771133	267865.074163	36.971623
1616.296171	268393.512704	36.976640
1617.734911	268916.350875	36.981658
1619.090653	269437.144543	36.986676
1620.901855	269965.000740	36.991693
1622.505643	270498.682416	36.996711
1624.543887	271021.114419	37.001728
1626.155711	271537.976635	37.006746
1627.777246	272064.515050	37.011764
1629.559750	272584.827837	37.016781
1630.994391	273107.356473	37.021799
1632.544575	273637.689277	37.026816
1634.272346	274162.936746	37.031834
1635.635601	274675.415083	37.036852
1637.515488	275174.928137	37.041869
1639.183278	275681.892866	37.046887
1640.865891	276180.064920	37.051904
1642.472422	276689.908344	37.056922
1643.724331	277190.537359	37.061940
1645.284018	277692.968962	37.066957
1646.407779	278216.555395	37.071975
1648.199830	278728.167522	37.076992
1649.775017	279246.876099	37.082010
1651.169137	279771.582841	37.087028
1652.792707	280300.645011	37.092045
1654.415875	280844.870931	37.097063
1656.272352	281376.381310	37.102080
1657.341960	281908.502719	37.107098
1658.572843	282458.631360	37.112116
1660.478094	282997.749773	37.117133
1662.336126	283539.770186	37.122151
1664.417081	284092.370052	37.127168
1666.125281	284641.676668	37.132186
1667.567820	285206.367821	37.137204
1669.603682	285747.208904	37.142221
1670.980634	286304.820140	37.147239
1672.888398	286868.387337	37.152256
1674.422239	287434.401894	37.157274
1675.839453	287989.028551	37.162292
1677.493855	288554.333204	37.167309
1679.105478	289132.495543	37.172327
1681.190893	289707.859517	37.177344
1682.579957	290279.856145	37.182362
1684.027518	290861.492940	37.187380
1686.073869	291429.566253	37.192397
1687.797018	292011.508206	37.197415
1689.407579	292595.675954	37.202432
1690.704022	293168.259646	37.207450
1692.925604	293757.655252	37.212468
1694.764116	294332.709563	37.217485
1696.452080	294917.336268	37.222503
1698.698254	295497.118304	37.227520
1700.463854	296079.516705	37.232538
1702.121101	296656.926384	37.237556
1703.828024	297235.340903	37.242573
1705.717897	297825.355004	37.247591
1707.446037	298394.667128	37.252608
1709.296112	298958.444614	37.257626
1710.922381	299547.045107	37.262644
1713.006282	300121.191269	37.267661
1714.302172	300691.679899	37.272679
1715.872160	301287.899297	37.277696
1717.583537	301863.722607	37.282714
1719.102959	302451.892225	37.287732
1721.019481	303047.154962	37.292749
1722.330342	303633.523200	37.297767
1724.224511	304222.712301	37.302784
1726.088665	304815.890027	37.307802
1727.441237	305416.767481	37.312820
1729.425233	306001.054208	37.317837
1731.158089	306609.505510	37.322855
1732.844037	307189.719379	37.327872
1734.277713	307803.976847	37.332890
1735.754251	308408.292966	37.337908
1737.691746	309014.306502	37.342925
1738.810163	309629.110812	37.347943
1741.129116	310238.150888	37.352960
1742.787625	310850.393671	37.357978
1744.688765	311460.103085	37.362996
1746.789180	312070.105144	37.368013
1748.295016	312680.327584	37.373031
1750.145521	313262.808178	37.378048
1751.648054	313864.032188	37.383066
1753.611459	314453.773410	37.388084
1755.306078	315030.425625	37.393101
1757.207777	315616.155683	37.398119
1758.706973	316189.072899	37.403136
1760.862839	316779.017971	37.408154
1762.215315	317365.332583	37.413172
1764.551495	317937.818644	37.418189
1766.785269	318517.096916	37.423207
1768.506249	319111.563696	37.428224
1770.116267	319690.122630	37.433242
1771.631856	320268.997015	37.438260
1773.526243	320860.652412	37.443277
1775.391883	321464.622439	37.448295
1777.129830	322050.173790	37.453312
1778.767777	322646.857916	37.458330
1780.134265	323242.286474	37.463348
1782.172931	323842.270648	37.468365
1783.315781	324457.580663	37.473383
1784.963840	325064.955781	37.478400
1786.938600	325677.019158	37.483418
1788.158170	326311.468131	37.488436
1790.256697	326938.199518	37.493453
1791.817357	327570.852827	37.498471
1793.546101	328202.151617	37.503488
1795.491634	328833.382669	37.508506
1797.022347	329474.500895	37.513524
1798.922553	330115.906683	37.518541
1800.619952	330776.989288	37.523559
1802.730196	331426.927223	37.528576
1804.563764	332077.538166	37.533594
1806.161199	332726.733591	37.538612
1808.289410	333382.129974	37.543629
1810.211322	334036.435729	37.548647
1811.484440	334681.752520	37.553664
1813.500623	335345.648674	37.558682
1815.169909	336016.854298	37.563700
1817.216771	336672.707330	37.568717
1818.960283	337349.443529	37.573735
1820.624700	338019.431837	37.578752
1822.997704	338667.895690	37.583770
1824.647181	339349.394035	37.588788
1826.684219	340024.118188	37.593805
1828.348694	340691.279919	37.598823
1830.171862	341354.320070	37.603840
1832.270756	342029.591305	37.608858
1834.593515	342696.795680	37.613876
1836.599999	343352.722870	37.618893
1837.775633	344027.256303	37.623911
1839.814693	344697.145515	37.628928
1841.880857	345359.939708	37.633946
1843.407478	346037.813768	37.638964
1845.341778	346710.966370	37.643981
1846.762188	347385.920024	37.648999
1848.664566	348077.915720	37.654016
1850.492876	348767.832281	37.659034
1851.832109	349444.876036	37.664052
1854.073922	350136.049009	37.669069
1855.519664	350831.073395	37.674087
1857.214828	351532.821804	37.679104
1858.898674	352225.095390	37.684122
1860.591330	352947.580626	37.689140
1862.147583	353652.617555	37.694157
1864.030262	354365.557391	37.699175
1865.943938	355079.216332	37.704192
1868.128417	355789.114037	37.709210
1869.767718	356503.251380	37.714228
1871.550032	357222.326525	37.719245
1873.250245	357920.773970	37.724263
1875.312445	358618.185880	37.729280
1876.739683	359312.493835	37.734298
1878.593080	359996.646890	37.739316
1880.249639	360702.894856	37.744333
1882.547124	361416.484174	37.749351
1884.270848	362142.486014	37.754368
1886.636454	362840.359416	37.759386
1888.244173	363544.003229	37.764404
1890.036738	364263.181227	37.769421
1891.987996	364970.193281	37.774439
1893.503217	365690.557851	37.779456
1895.593012	366416.598315	37.784474
1897.727496	367150.634049	37.789492
1899.498395	367877.156132	37.794509
1901.499639	368609.131002	37.799527
1903.463565	369334.350317	37.804544
1905.427078	370066.176236	37.809562
1906.996292	370809.188324	37.814580
1909.472227	371536.005184	37.819597
1911.163546	372275.391110	37.824615
1913.253364	373008.634316	37.829632
1915.385489	373757.403593	37.834650
1917.266308	374507.923444	37.839668
1919.172510	375245.209501	37.844685
1921.654904	375986.088083	37.849703
1923.152449	376739.439230	37.854720
1925.464487	377485.285204	37.859738
1927.257386	378242.460848	37.864756
1929.441498	378966.587665	37.869773
1931.477162	379702.287567	37.874791
1933.626645	380453.649928	37.879808
1935.848599	381178.966249	37.884826
1938.188387	381930.340557	37.889844
1940.282685	382663.303965	37.894861
1941.955822	383390.793024	37.899879
1943.914523	384127.423239	37.904896
1946.103228	384877.564185	37.909914
1948.023507	385612.696847	37.914932
1949.758809	386337.220013	37.919949
1951.886428	387080.702859	37.924967
1953.426510	387834.305250	37.929984
1955.790923	388564.936729	37.935002
1957.682369	389314.364474	37.940020
1959.740775	390055.152848	37.945037
1961.626975	390797.447866	37.950055
1963.428723	391543.744505	37.955072
1965.346493	392299.408742	37.960090
1967.312113	393045.591501	37.965108
1969.437396	393786.457379	37.970125
1971.591433	394547.350506	37.975143
1973.154182	395291.314288	37.980160
1975.791829	396035.538707	37.985178
1977.964084	396790.390607	37.990196
1979.387671	397536.628211	37.995213
1981.527651	398289.293132	38.000231
1983.167343	399046.633961	38.005248
1985.168042	399801.310737	38.010266
1987.333417	400556.346346	38.015284
1989.289134	401304.351896	38.020301
1991.016274	402074.219860	38.025319
1992.727020	402845.793067	38.030336
1994.988016	403595.766572	38.035354
1996.608199	404379.324283	38.040372
1998.194860	405139.098403	38.045389
2000.474837	405902.538321	38.050407
2002.574168	406694.263308	38.055424
2004.470802	407450.528392	38.060442
2006.347947	408200.594143	38.065460
2008.287869	408955.240071	38.070477
2010.708901	409695.826707	38.075495
2012.288346	410441.472062	38.080512
2014.500879	411196.694991	38.085530
2016.538607	411950.329689	38.090548
2018.321021	412713.383297	38.095565
2020.450232	413460.146275	38.100583
2022.885238	414216.741862	38.105600
2025.121000	414966.129827	38.110618
2027.157150	415726.218012	38.115636
2028.614327	416489.064367	38.120653
2030.542543	417235.094859	38.125671
2032.529138	418019.767535	38.130688
2034.590599	418791.209403	38.135706
2036.746264	419578.440529	38.140724
2038.312395	420363.136253	38.145741
2040.736941	421136.675919	38.150759
2042.624316	421927.677014	38.155776
2044.691334	422694.112293	38.160794
2047.186003	423491.395660	38.165812
2048.552110	424299.246163	38.170829
2050.439200	425091.438455	38.175847
2052.118868	425905.615868	38.180864
2054.571905	426717.258897	38.185882
2056.236992	427542.878438	38.190900
2058.217594	428360.468746	38.195917
2060.296669	429184.495806	38.200935
2062.086578	430014.921487	38.205952
2064.056334	430853.540813	38.210970
2066.290087	431701.958878	38.215988
2068.190553	432539.112671	38.221005
2070.519647	433393.377190	38.226023
2072.410266	434236.749204	38.231040
2074.352228	435090.357602	38.236058
2076.428038	435952.162881	38.241076
2078.684356	436831.620982	38.246093
2080.866900	437673.858148	38.251111
2083.014819	438534.036479	38.256128
2085.353010	439404.930405	38.261146
2087.636044	440259.757924	38.266164
2089.937007	441125.379325	38.271181
2091.987359	441979.066618	38.276199
2094.103076	442852.950505	38.281216
2096.223315	443699.273982	38.286234
2098.734369	444558.807406	38.291252
2100.849195	445436.485295	38.296269
2103.072766	446284.564343	38.301287
2105.152973	447156.310218	38.306304
2107.171196	448007.846678	38.311322
2109.066612	448867.969464	38.316340
2111.414261	449750.189651	38.321357
2113.710529	450613.110242	38.326375
2115.288239	451487.191366	38.331392
2117.467647	452353.702311	38.336410
2119.709350	453219.712229	38.341428
2121.462029	454090.824456	38.346445
2123.882714	454966.847394	38.351463
2125.763882	455864.818948	38.356480
2128.096093	456742.399796	38.361498
2130.165956	457614.576109	38.366516
2132.098349	458496.597797	38.371533
2134.067203	459391.721173	38.376551
2136.892645	460271.951418	38.381568
2139.415594	461130.251871	38.386586
2141.495236	462014.826453	38.391604
2143.365078	462892.572155	38.396621
2145.662411	463755.296674	38.401639
2147.788712	464607.498114	38.406656
2149.723216	465452.820363	38.411674
2151.886897	466292.711025	38.416692
2153.739979	467151.569861	38.421709
2156.188230	467999.174325	38.426727
2158.290322	468858.675070	38.431744
2160.368969	469693.531389	38.436762
2162.585579	470555.616220	38.441780
2164.849760	471412.702648	38.446797
2167.201212	472263.571971	38.451815
2169.067148	473118.121225	38.456832
2171.213903	473974.808750	38.461850
2173.172629	474853.464998	38.466868
2175.072269	475729.210470	38.471885
2177.267983	476598.955877	38.476903
2179.219211	477481.935677	38.481920
2181.555690	478361.173243	38.486938
2183.966651	479255.610452	38.491956
2185.535290	480148.122942	38.496973
2187.999218	481040.292946	38.501991
2189.981951	481946.235162	38.507008
2192.160985	482846.848088	38.512026
2195.301456	483741.097221	38.517044
2197.280466	484660.387051	38.522061
2199.757539	485575.609477	38.527079
2202.005128	486478.301809	38.532096
2203.973109	487384.074232	38.537114
2205.942716	488307.166543	38.542132
2208.160665	489225.676964	38.547149
2210.188798	490136.700037	38.552167
2212.531911	491061.302768	38.557184
2214.448274	491988.955328	38.562202
2217.178265	492917.433698	38.567220
2218.941131	493855.711551	38.572237
2221.290259	494784.808563	38.577255
2223.388480	495741.701268	38.582272
2225.674611	496673.784539	38.587290
2227.886763	497627.525289	38.592308
2229.748748	498580.462950	38.597325
2231.943412	499537.126308	38.602343
2234.033580	500503.690754	38.607360
2236.068756	501479.389514	38.612378
2238.370677	502436.374237	38.617396
2240.349360	503418.929737	38.622413
2242.570446	504403.404416	38.627431
2244.420017	505394.942191	38.632448
2246.945149	506393.974049	38.637466
2249.334296	507367.955630	38.642484
2251.401755	508388.019261	38.647501
2253.647088	509360.997485	38.652519
2255.782131	510365.496638	38.657536
2258.160420	511372.464085	38.662554
2260.536497	512379.620647	38.667572
2262.641935	513387.514359	38.672589
2265.085888	514384.753721	38.677607
2267.812728	515392.064690	38.682624
2269.991164	516410.741288	38.687642
2272.326893	517406.345683	38.692660
2274.880046	518411.072506	38.697677
2277.585843	519405.782745	38.702695
2279.414192	520419.770634	38.707712
2281.515948	521423.419312	38.712730
2284.131785	522416.640462	38.717748
2286.403938	523439.424247	38.722765
2288.744119	524451.600490	38.727783
2290.885196	525447.875989	38.732800
2292.999635	526466.452526	38.737818
2295.453118	527466.068965	38.742836
2297.237832	528453.743759	38.747853
2299.440796	529438.867328	38.752871
2301.535948	530428.978743	38.757888
2303.968679	531410.308490	38.762906
2306.296712	532396.121449	38.767924
2308.034505	533400.944648	38.772941
2310.370388	534397.646973	38.777959
2312.908337	535394.298363	38.782976
2315.076173	536411.578485	38.787994
2317.096995	537401.785385	38.793012
2319.276767	538425.867300	38.798029
2321.953428	539442.950810	38.803047
2324.277363	540471.291422	38.808064
2326.130964	541509.396414	38.813082
2328.756442	542529.488701	38.818100
2330.554337	543578.469570	38.823117
2332.919395	544616.313073	38.828135
2335.136912	545670.753263	38.833152
2337.610743	546730.403136	38.838170
2340.046538	547792.241952	38.843188
2342.331363	548855.633775	38.848205
2344.398613	549916.264536	38.853223
2346.451634	550987.022885	38.858240
2348.927129	552081.106885	38.863258
2351.548114	553169.650147	38.868276
2353.971197	554257.837548	38.873293
2356.268241	555349.929381	38.878311
2359.086711	556440.942450	38.883328
2361.324961	557535.983295	38.888346
2363.823627	558620.540155	38.893364
2366.317694	559723.802271	38.898381
2368.193686	560823.306715	38.903399
2371.282836	561922.017700	38.908416
2373.952663	563025.880666	38.913434
2376.358720	564110.305662	38.918452
2379.326792	565206.904044	38.923469
2381.594539	566302.872992	38.928487
2384.252028	567385.628822	38.933504
2386.682151	568485.404398	38.938522
2388.954490	569582.250481	38.943540
2391.374513	570686.308723	38.948557
2393.850345	571781.829030	38.953575
2396.319225	572873.391454	38.958592
2398.444552	573976.611698	38.963610
2400.854855	575082.750479	38.968628
2403.216209	576173.093147	38.973645
2405.270116	577280.603476	38.978663
2408.362938	578393.815537	38.983680
2410.437464	579497.112482	38.988698
2412.908167	580607.670883	38.993716
2415.558273	581719.053369	38.998733
2418.006619	582833.529057	39.003751
2420.139353	583949.159584	39.008768
2422.557898	585060.028020	39.013786
2425.163652	586161.688809	39.018804
2427.769212	587285.110312	39.023821
2430.231229	588399.678119	39.028839
2432.788350	589508.713602	39.033856
2435.321392	590615.445519	39.038874
2437.829747	591740.874420	39.043892
2440.142651	592852.498163	39.048909
2442.709484	593958.815032	39.053927
2445.169250	595078.575070	39.058944
2447.136017	596208.831654	39.063962
2449.654539	597307.428609	39.068980
2451.987608	598431.149470	39.073997
2454.306081	599563.129394	39.079015
2456.967210	600671.554860	39.084032
2459.206047	601769.478193	39.089050
2461.550022	602848.302768	39.094068
2464.002155	603947.686711	39.099085
2466.251862	605038.588469	39.104103
2468.644409	606145.782006	39.109120
2470.499429	607239.442567	39.114138
2472.899648	608335.961255	39.119156
2475.624137	609469.252725	39.124173
2477.873701	610584.545183	39.129191
2480.490844	611706.321220	39.134208
2482.887423	612840.428715	39.139226
2485.088789	613966.749957	39.144244
2487.436956	615100.636184	39.149261
2490.114245	616234.502621	39.154279
2492.596697	617386.588147	39.159296
2495.088381	618547.452501	39.164314
2497.339537	619706.784170	39.169332
2500.165270	620854.450402	39.174349
2502.843886	622016.566605	39.179367
2505.534289	623177.607256	39.184384
2507.790748	624356.286854	39.189402
2510.504805	625520.071231	39.194420
2512.645775	626706.158958	39.199437
2514.832716	627893.157348	39.204455
2517.074250	629076.268600	39.209472
2519.411590	630294.346740	39.214490
2522.031522	631498.904033	39.219508
2524.350953	632712.512405	39.224525
2526.308089	633941.419850	39.229543
2528.851125	635170.836067	39.234560
2531.290016	636408.861189	39.239578
2534.444839	637637.637115	39.244596
2536.822531	638883.963570	39.249613
2538.979430	640139.109052	39.254631
2542.229065	641380.799444	39.259648
2544.469696	642633.731559	39.264666
2547.354800	643885.755979	39.269684
2549.884714	645150.853223	39.274701
2552.715481	646409.061062	39.279719
2555.667576	647656.671182	39.284736
2557.924159	648922.490367	39.289754
2560.785650	650177.083361	39.294772
2563.174966	651440.868875	39.299789
2565.767087	652714.877937	39.304807
2568.449212	653981.334075	39.309824
2570.703061	655246.354094	39.314842
2573.295610	656512.850628	39.319860
2576.136001	657794.486602	39.324877
2578.545217	659077.271814	39.329895
2581.156417	660349.347760	39.334912
2583.748490	661640.282763	39.339930
2586.282580	662929.662008	39.344948
2588.617922	664200.682539	39.349965
2591.290223	665487.557689	39.354983
2594.352322	666769.120255	39.360000
2596.970580	668060.089288	39.365018
2600.412995	669321.343032	39.370036
2603.128011	670604.886748	39.375053
2605.599718	671886.804863	39.380071
2608.145914	673149.190219	39.385088
2610.606667	674438.472877	39.390106
2613.208750	675717.064232	39.395124
2615.819679	676995.479644	39.400141
2618.614910	678271.900169	39.405159
2621.285306	679541.655360	39.410176
2623.258164	680828.645239	39.415194
2625.847552	682100.000998	39.420212
2628.843306	683371.561451	39.425229
2631.204440	684635.052963	39.430247
2633.585111	685879.890814	39.435264
2636.010609	687143.173870	39.440282
2638.409541	688387.914176	39.445300
2640.838446	689649.606515	39.450317
2643.261876	690912.215598	39.455335
2645.791226	692187.981226	39.460352
2648.322779	693467.634384	39.465370
2650.917172	694757.761965	39.470388
2653.372803	696037.456300	39.475405
2655.695411	697327.206606	39.480423
2658.356424	698632.484941	39.485440
2661.177581	699943.742476	39.490458
2663.231881	701262.616081	39.495476
2665.625442	702590.059581	39.500493
2667.633130	703943.684746	39.505511
2670.557205	705290.803270	39.510528
2672.956310	706655.687056	39.515546
2675.838791	708015.420623	39.520564
2678.500745	709393.997507	39.525581
2680.984116	710772.630247	39.530599
2683.431135	712159.217628	39.535616
2685.943940	713567.254596	39.540634
2688.644562	714961.612230	39.545652
2691.407969	716367.707715	39.550669
2694.215972	717794.444837	39.555687
2696.261207	719210.823860	39.560704
2699.465979	720653.683836	39.565722
2701.913859	722081.482236	39.570740
2704.840096	723523.891522	39.575757
2707.404039	724975.948997	39.580775
2710.051089	726431.840836	39.585792
2712.604886	727888.429852	39.590810
2715.708571	729341.704767	39.595828
2718.826201	730801.241093	39.600845
2721.443117	732265.242145	39.605863
2724.459340	733727.086082	39.610880
2727.020139	735204.098740	39.615898
2729.883481	736667.509853	39.620916
2732.884397	738142.182916	39.625933
2735.429629	739618.584372	39.630951
2738.558247	741082.921742	39.635968
2741.278163	742554.555949	39.640986
2743.998735	744032.279987	39.646004
2747.096513	745498.420926	39.651021
2749.808712	746975.742568	39.656039
2752.522312	748457.863551	39.661056
2755.129062	749927.645079	39.666074
2757.799110	751407.783458	39.671092
2760.861212	752891.713773	39.676109
2763.516401	754385.328054	39.681127
2766.326489	755863.507026	39.686144
2769.278991	757347.779644	39.691162
2772.141668	758826.215956	39.696180
2774.846413	760317.091468	39.701197
2777.693954	761816.411174	39.706215
2780.327298	763293.918133	39.711232
2783.240603	764789.931341	39.716250
2785.990859	766266.344466	39.721268
2789.057718	767751.069581	39.726285
2791.336980	769257.114706	39.731303
2794.719233	770743.355649	39.736320
2797.129017	772236.290479	39.741338
2799.976164	773720.695545	39.746356
2802.697081	775219.314612	39.751373
2805.477367	776730.388297	39.756391
2808.584542	778212.173367	39.761408
2811.539885	779698.248514	39.766426
2813.990672	781155.633722	39.771444
2817.084885	782611.294977	39.776461
2819.487626	784073.302739	39.781479
2822.071734	785514.920132	39.786496
2825.243603	786972.630708	39.791514
2827.634779	788423.700310	39.796532
2830.844181	789886.008151	39.801549
2833.078062	791363.321899	39.806567
2836.372443	792822.658083	39.811584
2838.905998	794304.454050	39.816602
2841.305791	795778.514594	39.821620
2844.482189	797266.732104	39.826637
2847.047574	798755.174422	39.831655
2849.802459	800254.331392	39.836672
2852.568046	801758.008651	39.841690
2855.300522	803268.753821	39.846708
2858.509385	804776.937448	39.851725
2860.686782	806305.992211	39.856743
2863.662812	807835.797117	39.861760
2866.412754	809375.905879	39.866778
2869.076114	810912.308303	39.871796
2872.202185	812460.112691	39.876813
2875.186590	814011.494951	39.881831
2877.692955	815571.000450	39.886848
2880.822992	817141.761386	39.891866
2883.571028	818704.600998	39.896884
2886.812159	820273.338977	39.901901
2889.997234	821845.425167	39.906919
2893.275929	823415.854965	39.911936
2896.206459	824997.577602	39.916954
2899.312733	826570.358098	39.921972
2902.151376	828143.683623	39.926989
2904.949352	829733.891643	39.932007
2907.907892	831318.666683	39.937024
2910.750686	832897.423526	39.942042
2913.392049	834477.290133	39.947060
2916.377013	836078.771302	39.952077
2919.065713	837687.399630	39.957095
2922.491855	839284.212277	39.962112
2925.184557	840884.250228	39.967130
2928.324308	842484.591166	39.972148
2931.096669	844084.103156	39.977165
2933.531549	845706.020215	39.982183
2936.873938	847330.287261	39.987200
2939.691904	848958.400219	39.992218
2942.419280	850573.377017	39.997236
2946.097528	852195.647705	40.002253
2949.136251	853811.482993	40.007271
2951.883611	855448.886909	40.012288
2955.289423	857056.242556	40.017306
2958.141233	858702.084178	40.022324
2960.789358	860319.191931	40.027341
2963.505531	861944.492902	40.032359
2966.535285	863587.343363	40.037376
2969.428733	865230.063324	40.042394
2972.510114	866869.400032	40.047412
2975.690283	868499.653486	40.052429
2978.438843	870139.221862	40.057447
2981.230923	871784.822474	40.062464
2984.724029	873435.565995	40.067482
2987.355078	875071.769001	40.072500
2990.442174	876707.446355	40.077517
2993.395225	878361.650821	40.082535
2996.133087	880010.979392	40.087552
2999.147084	881675.846300	40.092570
3002.069709	883326.436579	40.097588
3005.069196	884978.093777	40.102605
3008.050847	886638.364258	40.107623
3010.538975	888263.385252	40.112640
3013.581902	889886.989813	40.117658
3016.064153	891504.536239	40.122676
3019.196062	893122.678283	40.127693
3022.205480	894757.743820	40.132711
3025.102713	896390.527919	40.137728
3028.131730	898009.809446	40.142746
3030.452571	899661.027121	40.147764
3033.894278	901323.042003	40.152781
3036.658722	902994.212807	40.157799
3039.660359	904655.797653	40.162816
3042.883461	906324.168045	40.167834
3046.008929	907999.753553	40.172852
3048.652596	909684.917731	40.177869
3051.711020	911367.674629	40.182887
3054.743528	913067.707921	40.187904
3058.332274	914760.205804	40.192922
3060.822398	916461.489910	40.197940
3063.979894	918173.276239	40.202957
3066.987159	919888.006664	40.207975
3070.017809	921608.431306	40.212992
3073.276721	923333.549496	40.218010
3076.069295	925063.565052	40.223028
3079.897132	926804.169001	40.228045
3082.742566	928536.030465	40.233063
3085.948335	930265.451010	40.238080
3089.209425	932019.878564	40.243098
3092.579647	933757.811938	40.248116
3095.829444	935482.462220	40.253133
3099.118716	937217.739271	40.258151
3101.791513	938972.444426	40.263168
3104.803914	940725.262962	40.268186
3107.902134	942492.680328	40.273204
3111.342487	944244.340954	40.278221
3113.837296	946026.425241	40.283239
3116.220229	947795.211548	40.288256
3120.021299	949589.507922	40.293274
3122.762031	951375.239701	40.298292
3125.946876	953157.699420	40.303309
3128.678115	954970.753621	40.308327
3131.673193	956832.045257	40.313344
3135.000560	958686.716624	40.318362
3137.662460	960554.099824	40.323380
3140.582276	962432.172845	40.328397
3143.728213	964315.751518	40.333415
3146.838425	966199.891650	40.338432
3149.883968	968100.121118	40.343450
3153.004457	970008.689429	40.348468
3155.828739	971905.548672	40.353485
3159.039259	973817.323422	40.358503
3161.881915	975738.369214	40.363520
3165.109130	977660.949015	40.368538
3168.123490	979594.610711	40.373556
3170.896073	981520.644563	40.378573
3174.315933	983460.431180	40.383591
3177.190615	985416.974998	40.388608
3180.409482	987362.378449	40.393626
3183.456402	989328.157209	40.398644
3186.649430	991297.705849	40.403661
3189.971826	993268.397705	40.408679
3192.647609	995231.321303	40.413696
3196.144202	997195.956327	40.418714
3198.954904	999189.835283	40.423732
3202.076865	1001181.504970	40.428749
3205.234791	1003168.003927	40.433767
3208.420257	1005158.844527	40.438784
3211.916796	1007141.950272	40.443802
3214.536208	1009135.845037	40.448820
3218.355454	1011080.095228	40.453837
3221.667633	1013031.991588	40.458855
3224.430713	1014977.975380	40.463872
3228.173535	1016914.121663	40.468890
3231.594781	1018854.975743	40.473908
3234.633767	1020801.896240	40.478925
3237.921852	1022734.077928	40.483943
3241.370843	1024699.497112	40.488960
3244.655456	1026637.582124	40.493978
3247.395630	1028585.034900	40.498996
3250.756260	1030543.101503	40.504013
3253.947941	1032503.211883	40.509031
3257.112360	1034481.647975	40.514048
3259.928730	1036463.393823	40.519066
3262.531394	1038436.754900	40.524084
3265.792039	1040438.900764	40.529101
3268.972420	1042467.030069	40.534119
3271.665178	1044487.370537	40.539136
3275.044163	1046519.186975	40.544154
3278.239397	1048559.143810	40.549172
3281.550694	1050609.779594	40.554189
3284.559516	1052670.188531	40.559207
3287.612309	1054736.455784	40.564224
3291.166823	1056817.244372	40.569242
3294.604517	1058899.572535	40.574260
3298.004513	1060986.401609	40.579277
3301.407679	1063066.966536	40.584295
3304.456227	1065153.807719	40.589312
3308.331257	1067256.603039	40.594330
3311.486835	1069369.642289	40.599348
3315.156223	1071458.489545	40.604365
3318.581211	1073565.839343	40.609383
3321.676025	1075676.262707	40.614400
3324.976479	1077787.177415	40.619418
3328.121402	1079911.944401	40.624436
3331.157723	1082022.794619	40.629453
3334.645929	1084153.504546	40.634471
3338.136605	1086293.034723	40.639488
3341.693934	1088425.309486	40.644506
3344.998558	1090568.059806	40.649524
3348.291678	1092702.327129	40.654541
3351.767295	1094850.708469	40.659559
3354.849769	1097014.330054	40.664576
3357.938611	1099166.499227	40.669594
3361.267065	1101322.538039	40.674612
3364.558088	1103491.443553	40.679629
3367.848301	1105650.332364	40.684647
3370.906567	1107835.434787	40.689664
3373.848771	1110007.105672	40.694682
3377.741929	1112200.099587	40.699700
3381.045683	1114396.193681	40.704717
3384.503615	1116585.469406	40.709735
3387.716766	1118792.989735	40.714752
3391.384576	1120983.852734	40.719770
3394.280625	1123199.009489	40.724788
3397.446984	1125390.521218	40.729805
3400.938703	1127589.142395	40.734823
3403.978341	1129812.533286	40.739840
3408.102444	1132030.077647	40.744858
3411.191436	1134255.015545	40.749876
3414.820603	1136457.434407	40.754893
3418.586984	1138680.121467	40.759911
3422.129735	1140894.816167	40.764928
3425.889175	1143106.562327	40.769946
3428.977218	1145322.694032	40.774964
3431.937996	1147537.727990	40.779981
3435.357833	1149755.724206	40.784999
3438.332370	1151968.190245	40.790004
3441.726097	1154102.745091	40.795008
3445.309180	1156194.214086	40.800013
3448.484223	1158228.751458	40.805018
3451.482538	1160191.071839	40.810023
3454.583407	1162073.366852	40.815028
3457.621991	1163871.592936	40.820032
3460.478510	1165615.787889	40.825037
3463.169803	1167256.540288	40.830042
3466.464666	1168825.149686	40.835047
3469.223101	1170317.622994	40.840052
3471.756425	1171720.487151	40.845056
3473.833724	1173062.044508	40.850061
3476.256158	1174334.763215	40.855066
3478.699933	1175525.175617	40.860071
3480.770889	1176639.715859	40.865076
3482.855286	1177704.181041	40.870080
3484.657381	1178698.871332	40.875085
3486.827875	1179626.450445	40.880090
3488.570053	1180494.146952	40.885095
3490.145911	1181306.372217	40.890100
3491.319095	1182070.532927	40.895104
3493.060225	1182779.620236	40.900109
3494.525991	1183426.361581	40.905114
3496.146232	1184043.546827	40.910119
3497.140951	1184601.868194	40.915124
3498.351245	1185120.490575	40.920128
3499.408968	1185602.684577	40.925133
3500.833599	1186046.211596	40.930138
3502.105972	1186433.204276	40.935143
3503.161614	1186790.675345	40.940148
3503.858176	1187117.714030	40.945152
3504.504324	1187418.412515	40.950157
3505.289213	1187665.289402	40.955162
3506.392318	1187893.956354	40.960167
3506.750811	1188107.693331	40.965172
3507.612728	1188283.357679	40.970176
3508.752498	1188443.082707	40.975181
3508.975582	1188571.461441	40.980186
3509.995474	1188673.666352	40.985191
3510.265893	1188759.448027	40.990196
3510.924119	1188803.051249	40.995200
3511.732574	1188852.645496	41.000205
3512.250908	1188866.754481	41.005210
3512.491321	1188849.136572	41.010215
3512.984496	1188842.475253	41.015220
3513.505513	1188807.044534	41.020224
3513.817555	1188758.769487	41.025229
3514.175279	1188688.395328	41.030234
3514.744876	1188615.353142	41.035239
3515.235533	1188514.684588	41.040244
3515.814776	1188404.128426	41.045248
3515.730426	1188290.952833	41.050253
3515.806394	1188151.142236	41.055258
3516.730552	1188005.171063	41.060263
3516.755725	1187845.146771	41.065268
3517.003453	1187673.798071	41.070272
3517.164274	1187502.269957	41.075277
3517.450261	1187324.321519	41.080282
3517.568750	1187131.537303	41.085287
3518.023806	1186932.672117	41.090292
3518.150569	1186717.208152	41.095296
3518.314313	1186498.061382	41.100301
3518.528335	1186291.405534	41.105306
3518.920738	1186049.724467	41.110311
3518.867794	1185807.164893	41.115316
3519.012865	1185558.071076	41.120320
3519.391722	1185322.190130	41.125325
3519.007152	1185068.080394	41.130330
3519.597397	1184794.606223	41.135335
3519.418613	1184544.764407	41.140340
3519.867699	1184277.401411	41.145344
3519.831781	1183998.249144	41.150349
3519.217809	1183714.472267	41.155354
3519.862465	1183432.825080	41.160359
3519.653665	1183157.137697	41.165364
3520.498845	1182863.192827	41.170368
3520.111922	1182573.387095	41.175373
3520.086724	1182277.011213	41.180378
3520.369566	1181974.261162	41.185383
3520.561548	1181667.178316	41.190388
3520.630549	1181370.076183	41.195392
3520.706345	1181053.844791	41.200397
3520.294781	1180743.794101	41.205402
3520.828351	1180416.150544	41.210407
3520.767956	1180116.173290	41.215412
3520.469791	1179791.357946	41.220416
3520.793080	1179482.617575	41.225421
3520.504454	1179161.999041	41.230426
3520.943413	1178819.672758	41.235431
3520.238219	1178511.514973	41.240436
3520.879377	1178188.045897	41.245440
3521.075485	1177856.717065	41.250445
3520.687288	1177521.412415	41.255450
3520.813947	1177195.516926	41.260455
3520.467649	1176871.657513	41.265460
3520.682079	1176533.834438	41.270464
3520.938210	1176200.882607	41.275469
3521.105755	1175872.258992	41.280474
3520.898006	1175542.639752	41.285479
3520.816240	1175207.323909	41.290484
3521.015191	1174858.273140	41.295488
3520.768048	1174524.542900	41.300493
3520.723834	1174179.445670	41.305498
3520.800021	1173833.834370	41.310503
3520.448695	1173502.224075	41.315508
3520.519117	1173161.094551	41.320512
3520.595275	1172828.616683	41.325517
3520.407573	1172485.316697	41.330522
3520.539387	1172147.033949	41.335527
3520.413279	1171817.071100	41.340532
3520.327901	1171483.307980	41.345536
3520.436043	1171132.796419	41.350541
3520.476329	1170787.271950	41.355546
3520.512912	1170449.649412	41.360551
3520.198187	1170120.176270	41.365556
3520.717209	1169779.223287	41.370560
3520.696841	1169433.336107	41.375565
3520.622902	1169092.058484	41.380570
3520.780634	1168731.847081	41.385575
3520.456738	1168390.753515	41.390580
3520.773215	1168038.017945	41.395584
3520.888587	1167700.110209	41.400589
3520.813510	1167336.348650	41.405594
3521.145546	1166974.760286	41.410599
3520.688221	1166631.025023	41.415604
3520.641803	1166275.209276	41.420608
3520.417398	1165937.149095	41.425613
3520.218870	1165583.766189	41.430618
3520.199241	1165228.913488	41.435623
3520.422688	1164889.861978	41.440628
3520.450153	1164541.848754	41.445632
3520.345108	1164192.417476	41.450637
3520.447717	1163841.134022	41.455642
3520.400240	1163482.672641	41.460647
3520.263980	1163139.316195	41.465652
3520.133161	1162805.383719	41.470656
3520.188221	1162433.229368	41.475661
3520.194461	1162091.859346	41.480666
3520.039776	1161740.760818	41.485671
3520.241321	1161400.542001	41.490676
3519.995262	1161053.097910	41.495680
3520.342997	1160701.090945	41.500685
3519.984954	1160349.271102	41.505690
3520.273519	1160005.450249	41.510695
3520.227297	1159667.995532	41.515700
3520.121074	1159303.018820	41.520704
3520.110280	1158959.651409	41.525709
3519.722045	1158613.014462	41.530714
3519.761736	1158259.570688	41.535719
3519.719490	1157912.168577	41.540724
3519.954270	1157567.724035	41.545728
3519.609482	1157227.891917	41.550733
3519.377692	1156882.722688	41.555738
3519.855565	1156536.373444	41.560743
3519.786564	1156199.739913	41.565748
3519.796102	1155838.003123	41.570752
3520.270014	1155498.964909	41.575757
3519.368697	1155155.022293	41.580762
3519.639522	1154800.456153	41.585767
3519.601038	1154460.773050	41.590772
3519.560696	1154116.052908	41.595776
3519.549960	1153770.642840	41.600781
3519.334333	1153436.979519	41.605786
3519.519190	1153079.188304	41.610791
3519.311888	1152738.475289	41.615796
3519.694098	1152394.424648	41.620800
3519.506084	1152049.025425	41.625805
3519.191332	1151706.559294	41.630810
3519.373722	1151357.740142	41.635815
3519.443304	1151020.846913	41.640820
3519.307649	1150674.307346	41.645824
3519.397144	1150328.181396	41.650829
3519.254724	1149982.733837	41.655834
3519.269804	1149640.741994	41.660839
3519.250559	1149299.396634	41.665844
3519.381376	1148954.783877	41.670848
3519.147376	1148618.544850	41.675853
3518.906765	1148281.527588	41.680858
3519.252472	1147935.202324	41.685863
3518.918713	1147596.356539	41.690868
3518.939228	1147254.967050	41.695872
3518.920939	1146901.053570	41.700877
3519.015234	1146570.884107	41.705882
3518.965342	1146225.269916	41.710887
3518.828051	1145895.285888	41.715892
3518.995310	1145552.056101	41.720896
3519.162148	1145216.008142	41.725901
3518.814579	1144878.791175	41.730906
3518.926432	1144533.798027	41.735911
3518.525346	1144189.340876	41.740916
3518.508959	1143847.926800	41.745920
3518.411134	1143524.235555	41.750925
3518.422133	1143193.015283	41.755930
3518.638032	1142849.696789	41.760935
3518.884258	1142517.352308	41.765940
3518.680967	1142182.689867	41.770944
3518.588959	1141844.952705	41.775949
3518.424413	1141510.146488	41.780954
3518.376645	1141171.789936	41.785959
3518.556783	1140844.378987	41.790964
3518.284515	1140510.855457	41.795968
3518.418338	1140162.347770	41.800973
3518.413352	1139839.649224	41.805978
3518.530063	1139483.698546	41.810983
3518.196680	1139159.684157	41.815988
3518.484543	1138836.876300	41.820992
3517.885298	1138504.798750	41.825997
3518.000580	1138168.026717	41.831002
3518.136839	1137838.728713	41.836007
3518.007662	1137519.041723	41.841012
3518.006667	1137184.409711	41.846016
3517.978538	1136862.103255	41.851021
3517.919098	1136538.168294	41.856026
3518.064296	1136197.943122	41.861031
3518.023071	1135881.086423	41.866036
3517.726242	1135550.768121	41.871040
3517.866976	1135225.485532	41.876045
3517.658206	1134907.648619	41.881050
3517.917500	1134568.914810	41.886055
3517.585996	1134258.752713	41.891060
3517.525563	1133930.764319	41.896064
3517.704325	1133606.421208	41.901069
3517.505518	1133294.755989	41.906074
3517.594892	1132963.548088	41.911079
3517.524507	1132648.023400	41.916084
3517.425943	1132317.946404	41.921088
3517.624529	1132000.533585	41.926093
3517.415995	1131684.309260	41.931098
3517.752813	1131354.385842	41.936103
3517.226742	1131040.361401	41.941108
3517.213681	1130716.824005	41.946112
3517.302343	1130403.706282	41.951117
3516.849060	1130088.663108	41.956122
3516.889731	1129771.713661	41.961127
3516.956265	1129460.065130	41.966132
3517.060848	1129150.959189	41.971136
3517.088100	1128831.769206	41.976141
3516.967379	1128519.240697	41.981146
3517.081758	1128200.854355	41.986151
3517.205853	1127889.009308	41.991156
3516.922329	1127573.884435	41.996160
3517.119429	1127264.939123	42.001165
3516.735955	1126944.562360	42.006170
3517.059527	1126629.471890	42.011175
3516.972776	1126321.089359	42.016180
3516.680165	1126005.017055	42.021184
3516.836216	1125695.131325	42.026189
3516.439418	1125377.611896	42.031194
3516.753076	1125073.943696	42.036199
3516.831411	1124778.765842	42.041204
3516.687909	1124460.198531	42.046208
3516.877280	1124149.551412	42.051213
3516.646221	1123847.520977	42.056218
3516.580529	1123520.319229	42.061223
3516.426489	1123218.050136	42.066228
3516.545936	1122910.959438	42.071232
3516.990237	1122601.036943	42.076237
3516.928553	1122296.225408	42.081242
3516.751057	1121973.231281	42.086247
3516.335807	1121668.632575	42.091252
3516.360470	1121368.419229	42.096256
3516.764957	1121052.414832	42.101261
3516.414867	1120744.610390	42.106266
3516.426894	1120433.776354	42.111271
3515.684208	1120134.953372	42.116276
3515.710436	1119837.606191	42.121280
3515.883078	1119541.837602	42.126285
3515.828090	1119246.185406	42.131290
3516.242412	1118949.296465	42.136295
3516.224718	1118652.748003	42.141300
3515.842668	1118352.813386	42.146304
3515.942435	1118052.973156	42.151309
3516.043465	1117754.164016	42.156314
3516.079558	1117454.300747	42.161319
3516.057146	1117161.958351	42.166324
3515.649863	1116847.268625	42.171328
3515.891008	1116565.142317	42.176333
3515.283311	1116267.891799	42.181338
3515.440711	1115960.872190	42.186343
3515.645170	1115691.477825	42.191348
3515.503134	1115399.821503	42.196352
3515.643589	1115105.719586	42.201357
3515.310663	1114819.687484	42.206362
3515.404768	1114519.269043	42.211367
3515.362932	1114246.219756	42.216372
3515.242819	1113949.809113	42.221376
3515.196181	1113653.942110	42.226381
3514.930801	1113367.630713	42.231386
3515.267309	1113076.436706	42.236391
3515.018167	1112811.645205	42.241396
3514.823234	1112530.141320	42.246400
3514.849018	1112242.958968	42.251405
3514.724152	1111968.472120	42.256410
3514.790027	1111681.062342	42.261415
3514.993134	1111403.249364	42.266420
3514.914845	1111130.810689	42.271424
3514.728824	1110846.927507	42.276429
3514.744125	1110566.144651	42.281434
3514.817111	1110290.203716	42.286439
3514.856767	1110011.773221	42.291444
3514.599520	1109717.727728	42.296448
3514.729354	1109448.223010	42.301453
3514.377078	1109180.406549	42.306458
3514.541677	1108898.462207	42.311463
3514.660583	1108622.618977	42.316468
3514.698386	1108355.174381	42.321472
3514.454115	1108075.163175	42.326477
3514.633779	1107808.336197	42.331482
3514.450585	1107529.336553	42.336487
3514.463530	1107266.519591	42.341492
3514.424805	1106993.673745	42.346496
3514.482953	1106715.355925	42.351501
3514.184321	1106440.519823	42.356506
3514.533708	1106156.300739	42.361511
3514.015013	1105895.318629	42.366516
3514.125050	1105623.429236	42.371520
3514.414763	1105357.990606	42.376525
3514.127677	1105094.448503	42.381530
3514.181724	1104818.420951	42.386535
3514.243047	1104569.313375	42.391540
3514.087656	1104293.006854	42.396544
3514.407304	1104029.312722	42.401549
3513.828563	1103747.125403	42.406554
3513.955374	1103478.277471	42.411559
3514.042245	1103227.097428	42.416564
3513.864614	1102954.069787	42.421568
3513.934204	1102691.784577	42.426573
3513.645151	1102442.349762	42.431578
3513.853543	1102176.481182	42.436583
3513.528336	1101918.045664	42.441588
3513.759555	1101655.205623	42.446592
3513.855162	1101381.957830	42.451597
3513.662289	1101119.926138	42.456602
3513.745606	1100869.879405	42.461607
3513.348407	1100614.547463	42.466612
3513.610015	1100341.315236	42.471616
3513.699840	1100092.856474	42.476621
3513.322849	1099840.926007	42.481626
3513.494881	1099569.963880	42.486631
3513.309270	1099317.212631	42.491636
3513.114045	1099068.562476	42.496640
3513.271151	1098809.420598	42.501645
3513.073378	1098561.034354	42.506650
3513.050181	1098317.006728	42.511655
3513.016288	1098083.297887	42.516660
3512.915292	1097832.854006	42.521664
3513.101136	1097572.691755	42.526669
3513.180084	1097337.114931	42.531674
3512.751157	1097092.907577	42.536679
3512.822025	1096856.163361	42.541684
3513.014923	1096602.648893	42.546688
3512.867028	1096350.326599	42.551693
3512.686232	1096114.165319	42.556698
3512.760492	1095873.263944	42.561703
3512.531013	1095628.766282	42.566708
3512.742246	1095384.759056	42.571712
3512.643293	1095145.288967	42.576717
3512.261011	1094912.840026	42.581722
3512.354663	1094668.724202	42.586727
3512.689021	1094438.337738	42.591732
3512.629206	1094200.733306	42.596736
3512.563804	1093953.931896	42.601741
3512.494598	1093710.278204	42.606746
3512.476690	1093480.483259	42.611751
3512.340166	1093244.955177	42.616756
3512.402142	1093007.948368	42.621760
3512.717741	1092763.135788	42.626765
3512.533208	1092528.063070	42.631770
3512.539851	1092272.844854	42.636775
3512.278142	1092045.135304	42.641780
3512.395355	1091802.609697	42.646784
3512.340237	1091563.452707	42.651789
3512.027756	1091329.593766	42.656794
3512.322126	1091111.711342	42.661799
3512.110762	1090873.794457	42.666804
3512.495530	1090631.459684	42.671808
3512.562753	1090395.008105	42.676813
3512.111826	1090172.709721	42.681818
3512.357577	1089934.293267	42.686823
3512.202401	1089698.901492	42.691828
3512.086730	1089464.163474	42.696832
3512.349028	1089231.747713	42.701837
3511.869982	1089001.359906	42.706842
3512.251069	1088762.965509	42.711847
3512.213985	1088527.886677	42.716852
3511.705327	1088304.754877	42.721856
3512.048310	1088076.012664	42.726861
3511.892712	1087847.151313	42.731866
3511.779785	1087615.782106	42.736871
3511.695283	1087393.022056	42.741876
3511.729771	1087170.520743	42.746880
3511.771690	1086946.571697	42.751885
3511.408105	1086732.263254	42.756890
3511.731928	1086487.741130	42.761895
3511.671060	1086283.140252	42.766900
3511.661824	1086069.322337	42.771904
3511.772813	1085836.882084	42.776909
3511.615136	1085608.885255	42.781914
3511.604197	1085376.061985	42.786919
3511.707096	1085162.094073	42.791924
3511.703983	1084941.616595	42.796929
3511.692348	1084723.911693	42.801933
3511.399016	1084498.670765	42.806938
3511.297193	1084265.527317	42.811943
3511.450490	1084058.602365	42.816948
3511.511816	1083842.863620	42.821953
3511.476395	1083610.831763	42.826957
3511.145085	1083402.906954	42.831962
3511.302073	1083177.633061	42.836967
3510.865290	1082973.832629	42.841972
3510.963255	1082763.415275	42.846977
3511.215663	1082546.634685	42.851981
3510.825472	1082346.159724	42.856986
3511.079684	1082130.896814	42.861991
3511.251254	1081922.448991	42.866996
3511.076631	1081705.417508	42.872001
3511.243989	1081486.018909	42.877005
3511.114747	1081286.900819	42.882010
3510.753514	1081070.354401	42.887015
3510.823698	1080849.699094	42.892020
3510.685250	1080648.832389	42.897025
3511.156400	1080435.865233	42.902029
3510.493959	1080237.756032	42.907034
3510.849142	1080027.478480	42.912039
3510.766512	1079817.264927	42.917044
3510.235938	1079608.076602	42.922049
3510.423496	1079422.176057	42.927053
3510.393154	1079237.072765	42.932058
3510.480437	1079020.275057	42.937063
3510.412326	1078827.966631	42.942068
3510.594104	1078629.563968	42.947073
3510.612106	1078423.215004	42.952077
3510.476265	1078217.747396	42.957082
3510.657987	1078014.523365	42.962087
3510.699863	1077823.025261	42.967092
3510.249410	1077611.827413	42.972097
3510.564912	1077422.094007	42.977101
3510.551437	1077223.864393	42.982106
3510.376063	1077004.053910	42.987111
3510.331825	1076812.534540	42.992116
3509.954893	1076624.039506	42.997121
3510.317236	1076421.878545	43.002125
3510.054187	1076224.037783	43.007130
3510.114702	1076027.192770	43.012135
3510.203722	1075844.067144	43.017140
3510.065535	1075649.353728	43.022145
3510.090156	1075444.427484	43.027149
3510.194685	1075263.968677	43.032154
3510.295528	1075065.545863	43.037159
3510.026229	1074869.001552	43.042164
3510.550422	1074665.596497	43.047169
3510.250595	1074472.788633	43.052173
3509.785877	1074279.616924	43.057178
3510.290063	1074081.668268	43.062183
3509.989410	1073885.862190	43.067188
3510.156030	1073703.228393	43.072193
3510.040714	1073520.634933	43.077197
3509.642360	1073327.322576	43.082202
3509.973008	1073140.800333	43.087207
3509.886758	1072940.986255	43.092212
3509.832602	1072755.667136	43.097217
3509.948277	1072560.609724	43.102221
3509.429098	1072373.432648	43.107226
3509.562596	1072192.579452	43.112231
3509.599740	1072012.504866	43.117236
3509.597892	1071816.287207	43.122241
3509.713651	1071638.109213	43.127245
3509.460689	1071455.085093	43.132250
3509.238914	1071282.044352	43.137255
3509.334960	1071098.085895	43.142260
3509.261505	1070909.632066	43.147265
3509.811338	1070728.854169	43.152269
3509.247929	1070551.137107	43.157274
3509.466524	1070371.843708	43.162279
3509.310475	1070197.988936	43.167284
3509.225194	1070013.062687	43.172289
3509.935026	1069834.824309	43.177293
3509.599020	1069656.944644	43.182298
3509.650262	1069469.574300	43.187303
3509.004950	1069289.714835	43.192308
3508.850255	1069105.634623	43.197313
3509.347147	1068929.516972	43.202317
3509.473576	1068764.607671	43.207322
3509.078926	1068580.741643	43.212327
3509.232307	1068411.298242	43.217332
3509.200989	1068238.803047	43.222337
3509.439685	1068060.776913	43.227341
3509.496921	1067884.601961	43.232346
3509.252097	1067696.450474	43.237351
3509.152170	1067517.693161	43.242356
3509.194613	1067356.409734	43.247361
3509.359586	1067170.384642	43.252365
3509.201042	1067003.257297	43.257370
3509.315343	1066821.075797	43.262375
3509.267462	1066656.997452	43.267380
3508.897777	1066476.519336	43.272385
3509.221819	1066304.578089	43.277389
3509.256464	1066136.142050	43.282394
3509.152800	1065946.368202	43.287399
3509.173954	1065782.348532	43.292404
3509.045866	1065599.493011	43.297409
3509.448594	1065417.890847	43.302413
3508.882199	1065247.987263	43.307418
3508.874199	1065078.756139	43.312423
3508.664958	1064899.161829	43.317428
3508.783911	1064735.768285	43.322433
3509.019198	1064572.062063	43.327437
3509.122882	1064404.331283	43.332442
3508.826275	1064236.757533	43.337447
3508.721878	1064063.469520	43.342452
3508.676591	1063908.546546	43.347457
3508.696733	1063739.846923	43.352461
3508.754500	1063580.855891	43.357466
3508.928203	1063397.299912	43.362471
3508.925318	1063236.672826	43.367476
3508.773209	1063061.436203	43.372481
3508.761165	1062894.737112	43.377485
3508.211607	1062716.667474	43.382490
3508.598389	1062544.501943	43.387495
3508.790600	1062395.368773	43.392500
3508.273758	1062230.850361	43.397505
3508.518702	1062072.458699	43.402509
3508.308136	1061913.848699	43.407514
3508.012596	1061754.477963	43.412519
3508.151529	1061599.074473	43.417524
3508.425858	1061438.349189	43.422529
3508.589857	1061272.438392	43.427533
3508.207839	1061117.203367	43.432538
3508.436893	1060958.685977	43.437543
3508.416301	1060802.323426	43.442548
3508.322298	1060653.190162	43.447553
3508.381818	1060487.946939	43.452557
3508.248716	1060331.011777	43.457562
3508.382731	1060165.072534	43.462567
3508.316816	1060015.243276	43.467572
3508.046370	1059853.502134	43.472577
3508.291450	1059691.960249	43.477581
3507.849953	1059545.743361	43.482586
3508.343277	1059383.188457	43.487591
3508.170935	1059238.941614	43.492596
3507.974267	1059080.536569	43.497601
3508.213645	1058921.091964	43.502605
3508.251862	1058774.390304	43.507610
3508.403188	1058611.002051	43.512615
3508.192213	1058460.865411	43.517620
3508.002613	1058309.083556	43.522625
3508.358529	1058158.170995	43.527629
3508.027060	1058004.188465	43.532634
3508.195704	1057845.302387	43.537639
3508.023050	1057687.142322	43.542644
3508.143834	1057522.281711	43.547649
3508.299672	1057376.583235	43.552653
3508.113006	1057231.804452	43.557658
3508.091379	1057076.685137	43.562663
3507.844728	1056913.890214	43.567668
3508.010513	1056763.259842	43.572673
3508.072339	1056614.473301	43.577677
3507.807000	1056467.567499	43.582682
3507.872659	1056324.746927	43.587687
3508.176509	1056172.921323	43.592692
3507.780281	1056010.124343	43.597697
3507.954807	1055877.971292	43.602701
3507.748189	1055717.640118	43.607706
3507.938683	1055564.563569	43.612711
3507.904987	1055428.386188	43.617716
3508.101905	1055270.481431	43.622721
3508.108508	1055113.470968	43.627725
3507.964559	1054970.360694	43.632730
3507.880430	1054801.693364	43.637735
3507.986501	1054656.509566	43.642740
3507.978833	1054514.907326	43.647745
3508.029872	1054363.169961	43.652749
3507.575907	1054208.715964	43.657754
3508.036276	1054053.239421	43.662759
3508.015585	1053906.514314	43.667764
3507.617345	1053753.966538	43.672769
3508.133094	1053609.748238	43.677773
3507.742516	1053473.388565	43.682778
3507.517964	1053314.725961	43.687783
3507.736933	1053169.195204	43.692788
3507.469218	1053023.933613	43.697793
3507.713273	1052876.366152	43.702797
3507.365138	1052744.706279	43.707802
3507.434799	1052593.206481	43.712807
3507.370420	1052451.849952	43.717812
3507.610881	1052310.053863	43.722817
3507.731214	1052173.674375	43.727821
3507.665394	1052032.210910	43.732826
3507.458830	1051871.478654	43.737831
3507.435011	1051742.248957	43.742836
3507.222182	1051608.996615	43.747841
3507.677533	1051458.173749	43.752845
3507.704458	1051324.007008	43.757850
3507.519832	1051179.744194	43.762855
3507.573830	1051026.467850	43.767860
3507.480227	1050888.837957	43.772865
3507.527002	1050751.085055	43.777869
3506.997149	1050625.288732	43.782874
3507.201404	1050482.101225	43.787879
3507.531581	1050347.282039	43.792884
3507.267252	1050198.858602	43.797889
3507.439131	1050057.305440	43.802893
3507.378159	1049929.100682	43.807898
3507.419234	1049785.922030	43.812903
3507.044937	1049645.509543	43.817908
3507.040379	1049515.549253	43.822913
3507.084614	1049370.526151	43.827917
3506.937843	1049241.837165	43.832922
3507.254695	1049106.603992	43.837927
3506.827964	1048986.446299	43.842932
3507.009913	1048853.834458	43.847937
3506.960816	1048716.143158	43.852941
3506.603168	1048590.079158	43.857946
3506.930564	1048450.968264	43.862951
3506.973875	1048330.236394	43.867956
3507.060764	1048187.298339	43.872961
3507.161838	1048062.111824	43.877965
3507.000580	1047937.062193	43.882970
3506.862949	1047803.030156	43.887975
3506.952704	1047676.678635	43.892980
3506.742676	1047548.346742	43.897985
3506.889613	1047421.690434	43.902989
3506.589031	1047286.997103	43.907994
3506.670263	1047160.152591	43.912999
3506.719596	1047035.530533	43.918004
3506.270556	1046919.096132	43.923009
3506.661933	1046791.612932	43.928013
3506.538509	1046666.142240	43.933018
3506.568751	1046541.994886	43.938023
3506.667306	1046413.103183	43.943028
3506.475921	1046286.283560	43.948033
3506.671323	1046158.142291	43.953037
3506.035721	1046050.988338	43.958042
3506.563756	1045936.206672	43.963047
3506.651252	1045815.895434	43.968052
3506.377590	1045686.855046	43.973057
3506.723527	1045559.544094	43.978061
3506.622966	1045448.814498	43.983066
3506.467602	1045323.994546	43.988071
3506.907137	1045202.356785	43.993076
3506.363483	1045078.850518	43.998081
3506.432343	1044956.689054	44.003085
3506.021966	1044843.487763	44.008090
3506.114463	1044725.083315	44.013095
3506.527810	1044598.318593	44.018100
3506.044373	1044477.106642	44.023105
3506.438967	1044360.769220	44.028109
3506.139062	1044258.740229	44.033114
3506.156215	1044146.902916	44.038119
3506.279721	1044026.643495	44.043124
3506.372201	1043913.823291	44.048129
3506.173132	1043793.418779	44.053133
3505.973151	1043686.823416	44.058138
3506.412886	1043555.394461	44.063143
3506.351647	1043437.084424	44.068148
3506.312552	1043328.717081	44.073153
3506.405845	1043210.086981	44.078157
3506.384128	1043095.337083	44.083162
3506.293823	1042971.033010	44.088167
3506.314529	1042852.503818	44.093172
3506.039539	1042730.060145	44.098177
3506.673762	1042624.756001	44.103181
3506.256581	1042514.019939	44.108186
3506.260064	1042382.345248	44.113191
3506.271356	1042273.176134	44.118196
3506.134684	1042151.759620	44.123201
3506.330937	1042043.908093	44.128205
3506.309026	1041927.491656	44.133210
3506.638916	1041796.039148	44.138215
3506.269015	1041669.916248	44.143220
3506.164446	1041558.723153	44.148225
3506.248354	1041444.501459	44.153229
3506.246319	1041341.790004	44.158234
3505.512334	1041218.905453	44.163239
3505.778549	1041118.851264	44.168244
3505.780389	1041012.557797	44.173249
3506.040633	1040902.257783	44.178253
3505.771417	1040794.941830	44.183258
3505.899624	1040684.562607	44.188263
3506.128047	1040584.215106	44.193268
3506.009174	1040467.880678	44.198273
3505.739461	1040346.929807	44.203277
3506.022537	1040250.432986	44.208282
3505.743358	1040136.630775	44.213287
3506.375730	1040026.928627	44.218292
3505.737386	1039921.009655	44.223297
3505.913703	1039802.486373	44.228301
3505.704138	1039707.801008	44.233306
3505.768028	1039587.938514	44.238311
3505.806936	1039482.382914	44.243316
3505.385428	1039385.407174	44.248321
3506.075776	1039285.636770	44.253325
3505.118105	1039181.206193	44.258330
3505.579375	1039068.806766	44.263335
3505.688727	1038972.606374	44.268340
3505.772529	1038870.318421	44.273345
3505.885752	1038767.927072	44.278349
3505.762581	1038657.452323	44.283354
3506.068557	1038545.551263	44.288359
3505.830256	1038448.625673	44.293364
3505.426093	1038340.414442	44.298369
3505.716058	1038233.150257	44.303373
3505.584441	1038136.781736	44.308378
3505.872603	1038030.287387	44.313383
3505.781638	1037921.049581	44.318388
3505.581811	1037815.211594	44.323393
3505.623502	1037711.652341	44.328397
3505.436481	1037615.187217	44.333402
3505.685321	1037506.465445	44.338407
3505.635187	1037418.096487	44.343412
3505.242004	1037329.879320	44.348417
3505.527152	1037216.504535	44.353421
3505.385137	1037112.674297	44.358426
3505.174451	1037021.327811	44.363431
3505.507329	1036926.215620	44.368436
3505.179464	1036817.188557	44.373441
3505.984620	1036709.906869	44.378445
3505.330096	1036615.435521	44.383450
3505.645486	1036519.352187	44.388455
3505.865304	1036423.863201	44.393460
3505.606724	1036313.847754	44.398465
3505.724653	1036210.538148	44.403469
3505.515497	1036113.276909	44.408474
3505.539571	1036006.980777	44.413479
3505.763477	1035902.680824	44.418484
3505.828975	1035798.695173	44.423489
3505.945719	1035688.025211	44.428493
3505.432451	1035590.127850	44.433498
3505.552052	1035486.901269	44.438503
3505.642940	1035392.189646	44.443508
3505.445760	1035293.461177	44.448513
3505.713268	1035174.437347	44.453517
3505.502866	1035087.895704	44.458522
3505.223476	1034989.465585	44.463527
3505.421689	1034890.084428	44.468532
3505.294458	1034789.690967	44.473537
3505.716881	1034686.109456	44.478541
3505.230576	1034603.281881	44.483546
3505.556096	1034503.292404	44.488551
3505.440697	1034414.402785	44.493556
3505.377758	1034310.120258	44.498561
3505.611367	1034207.141431	44.503565
3505.277067	1034117.025376	44.508570
3505.290959	1034013.401899	44.513575
3505.525512	1033916.512968	44.518580
3505.323731	1033827.047677	44.523585
3505.379528	1033716.832373	44.528589
3505.237088	1033632.288832	44.533594
3505.355010	1033529.316537	44.538599
3505.407185	1033433.416860	44.543604
3504.875209	1033341.966141	44.548609
3505.155280	1033234.316998	44.553613
3505.251207	1033142.759595	44.558618
3505.071668	1033053.278217	44.563623
3505.007086	1032960.970109	44.568628
3504.736582	1032872.952381	44.573633
3505.134778	1032777.952166	44.578637
3505.107474	1032702.085223	44.583642
3504.879936	1032605.539944	44.588647
3505.089353	1032517.631119	44.593652
3504.599106	1032430.320043	44.598657
3504.805969	1032324.697785	44.603661
3504.971181	1032248.502618	44.608666
3505.227068	1032164.742264	44.613671
3505.079461	1032074.949568	44.618676
3504.545445	1031980.379665	44.623681
3505.108959	1031877.206687	44.628685
3505.043496	1031810.432135	44.633690
3504.808643	1031720.067347	44.638695
3505.060014	1031630.395368	44.643700
3504.766124	1031539.553407	44.648705
3504.775934	1031439.173807	44.653709
3504.831927	1031364.630115	44.658714
3504.756545	1031266.778210	44.663719
3504.790598	1031181.006818	44.668724
3504.683117	1031104.647340	44.673729
3504.948548	1031015.253573	44.678733
3504.850729	1030942.568866	44.683738
3504.497828	1030841.076571	44.688743
3504.893864	1030750.979408	44.693748
3504.455298	1030679.218674	44.698753
3505.047520	1030596.637934	44.703757
3504.675177	1030517.409679	44.708762
3504.667867	1030432.504917	44.713767
3504.638779	1030342.664813	44.718772
3504.873863	1030269.819700	44.723777
3505.043632	1030174.619165	44.728781
3504.672851	1030093.351422	44.733786
3504.830708	1030010.639920	44.738791
3504.585688	1029930.123665	44.743796
3504.458873	1029852.975654	44.748801
3504.929011	1029767.013888	44.753805
3504.685546	1029691.335252	44.758810
3504.674960	1029608.451880	44.763815
3504.869470	1029532.989452	44.768820
3504.575718	1029442.597471	44.773825
3505.027975	1029352.662162	44.778829
3504.940542	1029266.203522	44.783834
3504.705815	1029179.574129	44.788839
3504.819106	1029098.986873	44.793844
3504.795485	1029010.673845	44.798849
3504.462222	1028915.728379	44.803853
3504.398220	1028840.202328	44.808858
3504.340897	1028770.581626	44.813863
3504.345266	1028706.566898	44.818868
3504.252275	1028612.835691	44.823873
3504.568337	1028535.015451	44.828877
3504.374625	1028460.474107	44.833882
3504.601561	1028387.218393	44.838887
3504.636413	1028310.700400	44.843892
3504.439727	1028226.277540	44.848897
3504.637987	1028138.592154	44.853901
3504.158729	1028080.751749	44.858906
3504.618117	1028008.130773	44.863911
3504.566488	1027916.802500	44.868916
3504.329986	1027830.249325	44.873921
3504.614200	1027763.078178	44.878925
3504.305634	1027684.670949	44.883930
3504.265298	1027603.699980	44.888935
3504.559409	1027530.034516	44.893940
3504.288945	1027446.871276	44.898945
3504.455270	1027374.871548	44.903949
3504.352071	1027297.587477	44.908954
3504.101485	1027221.585929	44.913959
3504.414271	1027135.319005	44.918964
3504.184329	1027075.780298	44.923969
3504.290749	1027002.332544	44.928973
3504.195044	1026930.370248	44.933978
3504.254611	1026852.375085	44.938983
3504.682119	1026776.062045	44.943988
3504.729161	1026710.176734	44.948993
3504.564749	1026637.350068	44.953997
3504.627347	1026544.624232	44.959002
3504.604945	1026464.602634	44.964007
3504.697093	1026387.273806	44.969012
3504.219944	1026311.200306	44.974017
3504.501338	1026222.792983	44.979021
3504.210536	1026163.254578	44.984026
3504.233960	1026075.274966	44.989031
3504.391391	1026014.789143	44.994036
3504.297942	1025929.927020	44.999041
3504.139877	1025848.465555	45.004045
3504.368185	1025789.806619	45.009050
3504.214271	1025714.156233	45.014055
3504.444644	1025628.170336	45.019060
3503.888658	1025560.045237	45.024065
3504.351157	1025488.263145	45.029069
3504.363227	1025420.430391	45.034074
3504.446766	1025339.793841	45.039079
3504.312312	1025278.476005	45.044084
3504.299827	1025195.527490	45.049089
3504.466324	1025113.129710	45.054093
3504.056955	1025038.675145	45.059098
3504.241975	1024964.509331	45.064103
3504.239434	1024904.425495	45.069108
3503.728854	1024837.156301	45.074113
3504.039550	1024761.901075	45.079117
3504.084394	1024694.441774	45.084122
3503.868760	1024618.786738	45.089127
3504.042789	1024549.172266	45.094132
3503.982976	1024479.401607	45.099137
3504.087683	1024407.567676	45.104141
3503.978458	1024344.975502	45.109146
3503.919136	1024266.285423	45.114151
3503.733753	1024204.964208	45.119156
3503.717131	1024148.557642	45.124161
3503.846902	1024077.006114	45.129165
3503.832671	1024022.536384	45.134170
3503.990167	1023949.524772	45.139175
3504.295487	1023886.665344	45.144180
3504.000164	1023823.516419	45.149185
3504.506172	1023749.572437	45.154189
3504.109470	1023681.107411	45.159194
3504.155588	1023607.140362	45.164199
3504.208508	1023533.655887	45.169204
3504.149153	1023460.576683	45.174209
3504.367193	1023384.445792	45.179213
3504.234895	1023329.019392	45.184218
3503.969801	1023247.537683	45.189223
3504.024251	1023175.987051	45.194228
3503.985443	1023102.512027	45.199233
3504.290148	1023032.081643	45.204237
3503.978779	1022972.318763	45.209242
3503.546946	1022898.227180	45.214247
3503.930312	1022850.854527	45.219252
3503.497864	1022799.931848	45.224257
3503.972947	1022731.311619	45.229261
3503.809308	1022658.626918	45.234266
3504.022099	1022592.084126	45.239271
3503.838807	1022531.519839	45.244276
3503.751252	1022469.775696	45.249281
3503.875224	1022400.142761	45.254285
3504.076206	1022341.355256	45.259290
3503.895489	1022264.790054	45.264295
3503.997613	1022199.812134	45.269300
3503.956698	1022137.377943	45.274305
3503.946605	1022066.502483	45.279309
3504.110098	1022007.620693	45.284314
3503.797376	1021936.502548	45.289319
3503.979969	1021871.895422	45.294324
3503.811734	1021815.005507	45.299329
3503.966107	1021740.511162	45.304333
3503.846955	1021683.805762	45.309338
3503.904071	1021614.755881	45.314343
3503.820858	1021549.703983	45.319348
3504.046698	1021478.103443	45.324353
3504.068517	1021402.365827	45.329357
3504.062698	1021347.577785	45.334362
3504.189679	1021275.021212	45.339367
3504.044095	1021216.182016	45.344372
3503.884037	1021141.343599	45.349377
3503.761923	1021072.122602	45.354381
3503.652036	1021012.499572	45.359386
3504.005946	1020950.569001	45.364391
3503.837239	1020890.469465	45.369396
3503.595144	1020824.174571	45.374401
3503.760751	1020758.490622	45.379405
3503.417769	1020711.316516	45.384410
3503.538058	1020646.608552	45.389415
3503.672529	1020581.994493	45.394420
3503.750877	1020525.244842	45.399425
3503.632245	1020470.369821	45.404429
3503.780450	1020406.527377	45.409434
3504.196606	1020332.359167	45.414439
3503.984078	1020287.972715	45.419444
3503.958661	1020215.136559	45.424449
3503.571114	1020148.178682	45.429453
3503.475841	1020085.051631	45.434458
3503.843532	1020020.877669	45.439463
3503.665577	1019958.441778	45.444468
3503.248823	1019913.504018	45.449473
3503.767269	1019854.056173	45.454477
3503.383462	1019793.204314	45.459482
3503.667061	1019725.645857	45.464487
3503.801975	1019676.056317	45.469492
3503.430267	1019631.205875	45.474497
3503.437710	1019561.556882	45.479501
3503.552574	1019503.432837	45.484506
3503.707162	1019443.652560	45.489511
3503.299952	1019384.255193	45.494516
3503.345429	1019326.625775	45.499521
3503.599929	1019263.916912	45.504525
3503.438502	1019214.372101	45.509530
3503.215694	1019159.404399	45.514535
3503.505552	1019097.075889	45.519540
3503.625517	1019042.341620	45.524545
3503.785580	1018987.018134	45.529549
3503.324385	1018932.572536	45.534554
3503.200447	1018879.526087	45.539559
3503.635911	1018832.013920	45.544564
3502.975580	1018779.442930	45.549569
3503.502464	1018721.922050	45.554573
3503.428650	1018666.827964	45.559578
3503.316485	1018609.023105	45.564583
3503.506746	1018559.608627	45.569588
3503.176948	1018500.965314	45.574593
3503.785865	1018436.539476	45.579597
3503.460624	1018387.014337	45.584602
3503.376839	1018328.716799	45.589607
3503.572775	1018281.821578	45.594612
3502.792869	1018228.294857	45.599617
3503.200528	1018185.633113	45.604621
3503.041646	1018123.076621	45.609626
3503.263794	1018077.339712	45.614631
3503.539899	1018034.213342	45.619636
3503.449611	1017974.651814	45.624641
3503.283308	1017924.320167	45.629645
3503.331921	1017875.020028	45.634650
3503.352584	1017828.829119	45.639655
3503.816998	1017766.554131	45.644660
3503.276183	1017707.840246	45.649665
3503.744195	1017644.690000	45.654669
3503.337702	1017601.866808	45.659674
3503.210395	1017529.400716	45.664679
3503.201164	1017482.726692	45.669684
3503.019040	1017443.940980	45.674689
3503.407109	1017386.817463	45.679693
3503.214857	1017341.142813	45.684698
3503.278938	1017287.371057	45.689703
3503.140650	1017230.235597	45.694708
3503.128359	1017190.158595	45.699713
3503.163005	1017124.744824	45.704717
3503.187035	1017080.973340	45.709722
3502.888566	1017046.474065	45.714727
3503.156777	1016988.492823	45.719732
3502.496569	1016941.630374	45.724737
3503.122172	1016888.538705	45.729741
3503.322963	1016852.597321	45.734746
3503.198281	1016805.257332	45.739751
3503.159163	1016752.856167	45.744756
3502.976584	1016703.972033	45.749761
3503.003768	1016651.170790	45.754765
3503.085287	1016611.850639	45.759770
3503.208277	1016567.573586	45.764775
3503.054535	1016509.656901	45.769780
3502.944666	1016463.088035	45.774785
3503.201056	1016420.728988	45.779789
3503.008419	1016374.658308	45.784794
3502.943839	1016325.848506	45.789799
3503.130429	1016274.473355	45.794804
3502.862293	1016206.769323	45.799809
3503.002239	1016096.580889	45.804813
3502.997609	1015941.569937	45.809818
3502.885670	1015706.199203	45.814823
3503.055815	1015415.536877	45.819828
3503.097804	1015071.195252	45.824833
3503.141076	1014653.628507	45.829837
3503.000395	1014188.775523	45.834842
3502.640882	1013636.623006	45.839847
3502.735643	1013035.103941	45.844852
3502.308650	1012354.350942	45.849857
3502.698264	1011623.256976	45.854861
3502.454524	1010811.340684	45.859866
3502.255506	1009935.265766	45.864871
3502.298390	1008984.668217	45.869876
3501.776814	1007958.088002	45.874881
3501.575287	1006869.046353	45.879885
3501.428653	1005726.594442	45.884890
3501.271860	1004480.523085	45.889895
3501.453598	1003159.016787	45.894900
3501.026536	1001759.746194	45.899905
3500.695136	1000282.245770	45.904909
3500.620299	998732.854007	45.909914
3500.400298	997094.437829	45.914919
3500.439188	995388.773380	45.919924
3499.868489	993583.687552	45.924929
3499.812957	991707.560783	45.929933
3499.729159	989746.760715	45.934938
3499.445655	987696.546325	45.939943
3499.226179	985572.880458	45.944948
3498.558817	983358.877095	45.949953
3498.539212	981056.986262	45.954957
3497.921968	978680.791607	45.959962
3497.853206	976225.223360	45.964967
3497.962387	973668.434623	45.969972
3496.817893	971035.867096	45.974977
3496.595663	968311.398494	45.979981
3496.227276	965529.547811	45.984986
3495.644752	962658.304192	45.989991
3495.347257	959690.003886	45.994996
3494.498781	956651.021329	46.000001
3494.003488	953562.753674	46.005005
3493.733262	950450.618505	46.010010
3492.880410	947242.558435	46.015015
3492.167343	943970.196450	46.020020
3492.219092	940615.200113	46.025025
3491.592540	937162.503467	46.030029
3491.130220	933647.026389	46.035034
3490.217319	930038.306500	46.040039
3489.944218	926359.162553	46.045044
3488.964736	922603.052519	46.050049
3488.631685	918751.417059	46.055053
3487.817011	914833.357333	46.060058
3487.138320	910825.705357	46.065063
3486.805817	906732.887279	46.070068
3485.686403	902572.791108	46.075073
3485.120183	898322.751866	46.080077
3484.326102	893995.779462	46.085082
3483.596798	889576.970595	46.090087
3483.167184	885093.419604	46.095092
3482.183169	880525.086505	46.100097
3481.230203	875852.310308	46.105101
3480.760150	871118.881656	46.110106
3479.825194	866312.511917	46.115111
3479.025457	861406.616185	46.120116
3477.990907	856436.383277	46.125121
3476.948268	851357.640497	46.130125
3476.384853	846208.103791	46.135130
3475.180986	840969.393481	46.140135
3474.347743	835670.854278	46.145140
3473.053741	830289.660749	46.150145
3472.637224	824807.640819	46.155149
3471.213327	819250.456674	46.160154
3470.576281	813618.319100	46.165159
3469.478731	807897.334378	46.170164
3468.282744	802097.634383	46.175169
3467.395382	796209.148182	46.180173
3466.452283	790237.037894	46.185178
3465.258553	784176.717803	46.190183
3464.159292	778039.451080	46.195188
3462.728798	771825.730254	46.200193
3461.895802	765517.040041	46.205197
3460.946631	759129.774026	46.210202
3459.663452	752680.104598	46.215207
3458.741030	746124.685144	46.220212
3457.134888	739475.633106	46.225217
3455.755706	732765.487979	46.230221
3454.740306	725971.122021	46.235226
3453.375785	719090.655236	46.240231
3452.423877	712106.174949	46.245236
3450.839556	705041.300887	46.250241
3449.186193	697913.800454	46.255245
3447.767176	690698.000181	46.260250
3446.237730	683418.609253	46.265255
3445.026600	676047.755000	46.270260
3443.580938	668586.825683	46.275265
3442.095063	661050.974864	46.280269
3440.720810	653451.118749	46.285274
3439.088620	645769.297091	46.290279
3438.130886	638000.295200	46.295284
3436.232772	630138.957846	46.300289
3434.479426	622205.884178	46.305293
3432.763323	614198.466731	46.310298
3431.160114	606131.680752	46.315303
3429.953411	597973.709249	46.320308
3428.139677	589731.108391	46.325313
3426.510722	581418.159176	46.330317
3424.861714	573038.381612	46.335322
3422.678884	564558.853104	46.340327
3421.016586	556022.803848	46.345332
3419.064328	547413.787680	46.350337
3417.744085	538717.963487	46.355341
3415.567890	529959.924166	46.360346
3413.833237	521132.147551	46.365351
3411.944497	512218.163788	46.370356
3409.893011	503230.149499	46.375361
3408.012040	494176.110780	46.380365
3405.929287	485050.779494	46.385370
3403.679869	475869.834773	46.390375
3401.608985	466610.077691	46.395380
3399.392321	457284.629109	46.400385
3397.467209	447876.795984	46.405389
3395.332099	438419.692207	46.410394
3392.741680	428907.976850	46.415399
3390.388843	419321.628818	46.420404
3388.272053	409652.173481	46.425409
3385.978029	399946.208788	46.430413
3383.199616	390165.293422	46.435418
3380.756242	380344.054299	46.440423
3378.048046	370463.563977	46.445428
3376.006414	360534.084387	46.450433
3373.136389	350530.928887	46.455437
3370.713836	340489.201485	46.460442
3367.834305	330399.731633	46.465447
3364.926093	320233.780946	46.470452
3362.169383	310042.411040	46.475457
3359.172893	299801.999921	46.480461
3356.316836	289517.086206	46.485466
3353.321708	279181.196429	46.490471
3350.387501	268810.450496	46.495476
3346.564380	258415.130179	46.500481
3343.552522	247971.926229	46.505485
3340.592597	237506.838723	46.510490
3337.058664	226946.635178	46.515495
3333.938417	216365.429459	46.520500
3330.034593	205834.732948	46.525505
3326.241266	195237.380963	46.530509
3322.983730	184649.163142	46.535514
3319.015951	174027.263866	46.540519
3314.915278	163401.591543	46.545524
3310.471722	152779.091659	46.550529
3306.281833	142134.814589	46.555533
3301.660524	131487.554605	46.560538
3296.795027	120854.517780	46.565543
3292.309304	110254.693097	46.570548
3287.094851	99664.677833	46.575553
3281.776780	89096.525047	46.580557
3276.206364	78555.816694	46.585562
3269.479404	68058.647093	46.590567
3262.834112	57624.421418	46.595572
3254.942228	47281.420501	46.600577
3245.663915	37058.332604	46.605581
3229.450540	27126.297040	46.610586
3195.583919	17870.580624	46.615591
3145.369691	9445.584436	46.620596
3073.631946	2325.146713	46.625601
2851.975168	417.596624	46.630605
2652.226681	413.400050	46.635610
2580.248633	402.206505	46.640615
2612.750899	366.715815	46.645620
2698.899771	362.130455	46.650625
2790.681305	362.547882	46.655629
2857.923195	365.545093	46.660634
2891.759180	365.702304	46.665639
2899.292363	355.520007	46.670644
2890.648282	352.975395	46.675649
2876.190936	354.663281	46.680653
2862.664906	351.174771	46.685658
2853.390866	359.551938	46.690663
2849.226439	341.501914	46.695668
2846.764983	340.018341	46.700673
2846.266347	338.068631	46.705677
2845.865976	330.799351	46.710682
2843.832668	337.102436	46.715687
2841.595300	339.836264	46.720692
2838.494115	346.223053	46.725697
2835.880154	333.881143	46.730701
2832.501566	325.989384	46.735706
2829.053946	325.345189	46.740711
2825.904819	324.458120	46.745716
2822.751393	334.058727	46.750721
2819.773786	326.603632	46.755725
2817.400649	320.315957	46.760730
2813.708880	332.936744	46.765735
2810.907492	317.356720	46.770740
2807.392421	322.236766	46.775745
2804.284932	325.369177	46.780749
2800.832605	316.385908	46.785754
2797.121485	320.651575	46.790759
2794.436434	316.048813	46.795764
2791.474730	325.102724	46.800769
2787.914221	311.043978	46.805773
2784.606036	305.233974	46.810778
2781.047885	319.453584	46.815783
2777.926451	308.155821	46.820788
2774.077426	312.937323	46.825793
2770.939440	309.682328	46.830797
2767.836259	308.153931	46.835802
2764.589597	304.943000	46.840807
2761.292866	302.840658	46.845812
2757.839064	312.036375	46.850817
2754.551952	302.190564	46.855821
2751.288578	299.318129	46.860826
2747.656959	306.479239	46.865831
2744.151048	293.061790	46.870836
2740.997674	299.254357	46.875841
2737.462976	304.479511	46.880845
2734.463893	301.865107	46.885850
2730.450129	296.416525	46.890855
2727.438334	297.323050	46.895860
2723.775989	296.212531	46.900865
2720.915034	288.646714	46.905869
2717.288184	293.021245	46.910874
2713.148778	296.555662	46.915879
2709.966914	295.889411	46.920884
2706.204241	297.182073	46.925889
2703.373784	302.064612	46.930893
2700.151598	294.416685	46.935898
2696.264400	298.218624	46.940903
2692.891593	300.056029	46.945908
2689.850633	290.222952	46.950913
2686.535783	293.018537	46.955917
2683.436356	302.150420	46.960922
2679.130899	298.112523	46.965927
2675.774052	282.553844	46.970932
2672.299379	295.682854	46.975937
2669.078062	295.301044	46.980941
2665.482788	286.254419	46.985946
2661.580161	293.568960	46.990951
2658.877937	282.817785	46.995956
2655.357580	284.019808	47.000961
2651.657444	283.202551	47.005965
2647.794479	281.304908	47.010970
2644.377364	280.674514	47.015975
2641.429672	275.244180	47.020980
2637.420484	277.987730	47.025985
2634.066601	272.677945	47.030989
2630.776304	268.123655	47.035994
2627.472590	280.902757	47.040999
2624.123665	279.377255	47.046004
2620.812902	268.295706	47.051009
2617.104902	272.782311	47.056013
2613.532717	271.926021	47.061018
2609.729827	275.062954	47.066023
2607.240268	270.369346	47.071028
2603.146879	270.718171	47.076033
2599.593794	279.434539	47.081037
2596.845359	274.422828	47.086042
2593.048304	278.469712	47.091047
2589.686321	268.612185	47.096052
2585.662846	268.696533	47.101057
2581.903843	272.107613	47.106061
2579.058787	274.892961	47.111066
2575.073529	270.119924	47.116071
2572.225487	266.798276	47.121076
2568.611494	270.071600	47.126081
2564.857305	259.074944	47.131085
2561.330826	270.395931	47.136090
2557.809499	266.306860	47.141095
2554.697245	266.329666	47.146100
2550.818009	275.439704	47.151105
2547.061081	274.476675	47.156109
2544.061710	266.123894	47.161114
2540.736730	259.481267	47.166119
2537.770349	258.691853	47.171124
2533.873109	271.039249	47.176129
2530.333645	255.800752	47.181133
2526.694525	263.166105	47.186138
2523.069965	267.625179	47.191143
2519.334567	258.219264	47.196148
2516.185677	259.905472	47.201153
2512.687115	263.771165	47.206157
2509.559906	258.227247	47.211162
2505.639627	259.260772	47.216167
2502.311732	262.511217	47.221172
2498.235639	264.631597	47.226177
2495.204633	259.097867	47.231181
2491.674464	258.671760	47.236186
2488.412077	261.191900	47.241191
2485.270147	247.516425	47.246196
2481.396753	249.431921	47.251201
2478.174031	258.417344	47.256205
2474.608950	244.748316	47.261210
2471.025415	265.302206	47.266215
2467.980036	243.953138	47.271220
2463.756387	264.026066	47.276225
2460.244625	258.802093	47.281229
2456.948325	254.122304	47.286234
2453.162384	258.604268	47.291239
2449.994810	252.987716	47.296244
2446.398569	246.090548	47.301249
2442.670579	259.027456	47.306253
2439.628946	251.007962	47.311258
2435.940558	245.225038	47.316263
2432.943295	248.982641	47.321268
2429.168220	258.873680	47.326273
2425.513998	246.682567	47.331277
2421.996737	250.216634	47.336282
2417.978355	250.069866	47.341287
2414.861040	246.570121	47.346292
2411.622044	257.212138	47.351297
2408.006487	252.494552	47.356301
2404.802950	244.100934	47.361306
2401.023148	257.468159	47.366311
2397.553859	242.636000	47.371316
2394.077572	248.550529	47.376321
2390.818426	240.602156	47.381325
2387.358807	243.969176	47.386330
2383.746951	241.476307	47.391335
2380.512202	239.037667	47.396340
2376.649609	243.222815	47.401345
2372.957270	236.054547	47.406349
2369.702753	236.469473	47.411354
2366.034922	237.327261	47.416359
2362.797444	242.805126	47.421364
2359.166764	236.660524	47.426369
2355.338162	239.735512	47.431373
2352.197522	247.630591	47.436378
2348.711024	244.280552	47.441383
2345.519848	238.364774	47.446388
2341.535126	231.391843	47.451393
2338.272503	231.142776	47.456397
2334.887456	234.415238	47.461402
2330.947001	250.521749	47.466407
2327.626778	234.489755	47.471412
2324.332500	237.136566	47.476417
2320.454245	240.069997	47.481421
2317.511799	234.319703	47.486426
2314.045232	233.000902	47.491431
2310.904455	227.487149	47.496436
2306.756240	242.374684	47.501441
2303.136628	237.776611	47.506445
2299.829693	235.391546	47.511450
2295.715456	242.806433	47.516455
2292.346663	232.488206	47.521460
2288.903922	239.331226	47.526465
2285.700582	229.336146	47.531469
2282.551769	230.158000	47.536474
2278.800409	239.107737	47.541479
2275.403840	223.567161	47.546484
2271.857362	227.598010	47.551489
2268.124924	236.535454	47.556493
2264.846156	227.784164	47.561498
2261.488196	235.324034	47.566503
2257.847984	228.611813	47.571508
2254.255197	237.982617	47.576513
2250.613674	236.060606	47.581517
2247.575716	224.581308	47.586522
2244.240398	234.546184	47.591527
2240.662093	237.747463	47.596532
2236.664583	237.086110	47.601537
2232.951034	237.969655	47.606541
2229.603393	227.418600	47.611546
2225.861404	237.123904	47.616551
2222.956067	215.757459	47.621556
2219.548063	225.633005	47.626561
2215.718691	221.792932	47.631565
2212.522749	229.516135	47.636570
2208.977727	232.409654	47.641575
2205.110976	227.344414	47.646580
2201.615605	225.790879	47.651585
2198.207035	229.260348	47.656589
2195.017980	223.439011	47.661594
2191.395815	224.679933	47.666599
2187.663936	218.765421	47.671604
2184.420643	234.057797	47.676609
2181.211699	226.602536	47.681613
2177.901352	220.827555	47.686618
2173.875188	227.498202	47.691623
2170.361718	222.451074	47.696628
2166.807769	229.965489	47.701633
2163.143511	235.127084	47.706637
2159.725527	221.557529	47.711642
2156.124027	225.450603	47.716647
2152.700908	222.606978	47.721652
2149.214143	224.465179	47.726657
2145.810083	227.844937	47.731661
2142.481713	226.825637	47.736666
2138.841413	233.016720	47.741671
2135.283132	224.498560	47.746676
2131.967522	220.772585	47.751681
2128.376423	220.515736	47.756685
2124.794236	220.007719	47.761690
2120.914051	230.816344	47.766695
2118.206433	223.058025	47.771700
2114.253936	223.878834	47.776705
2110.849842	221.643072	47.781709
2107.300978	233.194891	47.786714
2103.794988	227.932970	47.791719
2101.019643	209.526672	47.796724
2096.182810	218.593169	47.801729
2093.312957	226.761728	47.806733
2089.793528	229.117245	47.811738
2086.492564	214.090715	47.816743
2083.025940	212.051251	47.821748
2079.474035	224.723820	47.826753
2075.835757	218.510294	47.831757
2072.507126	210.516738	47.836762
2068.623415	217.718383	47.841767
2065.349652	210.729773	47.846772
2062.064356	216.005786	47.851777
2058.331332	222.334233	47.856781
2054.724368	217.656767	47.861786
2050.898053	214.749871	47.866791
2047.892041	206.935548	47.871796
2044.651570	212.521945	47.876801
2041.052586	217.543285	47.881805
2037.724460	213.407926	47.886810
2033.491717	216.780883	47.891815
2030.179753	219.127459	47.896820
2026.928408	209.800266	47.901825
2023.009629	212.553471	47.906829
2019.922185	211.169905	47.911834
2016.246439	218.903655	47.916839
2012.577279	206.581911	47.921844
2009.292484	214.409021	47.926849
2005.995504	215.239152	47.931853
2002.775811	204.717548	47.936858
1998.824998	206.091800	47.941863
1995.426086	206.113489	47.946868
1991.656523	206.249895	47.951873
1988.068893	209.362648	47.956877
1984.825307	200.149633	47.961882
1981.171841	220.118550	47.966887
1977.934674	206.979424	47.971892
1974.647007	201.050955	47.976897
1970.806370	216.198628	47.981901
1967.635037	203.608033	47.986906
1963.823213	204.296502	47.991911
1960.280969	217.532222	47.996916
1956.568448	214.397454	48.001921
1953.093318	209.923827	48.006925
1949.360643	210.308209	48.011930
1945.840361	211.900823	48.016935
1943.124409	211.949862	48.021940
1939.921639	210.051132	48.026945
1936.120060	207.675826	48.031949
1932.735758	210.818104	48.036954
1928.877255	213.904342	48.041959
1925.147663	203.123479	48.046964
1921.592486	212.285058	48.051969
1918.154863	208.562252	48.056973
1915.091945	206.520003	48.061978
1911.368283	202.064612	48.066983
1908.002193	204.255017	48.071988
1904.060809	202.825725	48.076993
1900.704570	203.239483	48.081997
1897.515489	203.285302	48.087002
1893.731357	201.043584	48.092007
1890.389950	198.154747	48.097012
1886.933998	201.369636	48.102017
1883.622650	202.183052	48.107021
1879.911038	196.365814	48.112026
1876.305580	200.685264	48.117031
1872.803349	201.976103	48.122036
1869.357557	204.473079	48.127041
1865.644385	196.081965	48.132045
1862.215823	194.990044	48.137050
1858.736549	213.196859	48.142055
1855.225127	204.301081	48.147060
1851.285149	203.900275	48.152065
1848.239327	205.259766	48.157069
1845.265636	203.480249	48.162074
1841.460792	196.806193	48.167079
1837.963229	195.558742	48.172084
1834.437327	194.684843	48.177089
1830.522853	197.464662	48.182093
1827.390705	198.171487	48.187098
1823.416680	203.658003	48.192103
1820.349408	193.957831	48.197108
1816.596897	198.293085	48.202113
1813.326561	213.389044	48.207117
1810.197845	197.001730	48.212122
1805.898008	198.967891	48.217127
1802.506513	195.031346	48.222132
1799.524146	200.862931	48.227137
1795.732410	206.769948	48.232141
1792.333196	201.234081	48.237146
1788.597635	208.318570	48.242151
1785.382108	198.399391	48.247156
1781.891505	187.686437	48.252161
1778.116179	201.949298	48.257165
1775.194621	199.277842	48.262170
1771.392855	205.758633	48.267175
1767.553887	210.411151	48.272180
1763.861450	194.304819	48.277185
1760.640877	188.651301	48.282189
1757.368421	198.708159	48.287194
1753.671900	203.263582	48.292199
1750.265816	196.324206	48.297204
1746.959599	197.306032	48.302209
1743.161252	202.245064	48.307213
1739.793689	188.352468	48.312218
1736.375045	193.770571	48.317223
1732.535615	196.088975	48.322228
1729.146472	198.939227	48.327233
1725.478015	199.317469	48.332237
1722.128874	183.145063	48.337242
1718.626632	199.750361	48.342247
1715.494992	198.063752	48.347252
1711.912158	201.803195	48.352257
1708.225071	193.477032	48.357261
1704.854822	190.125714	48.362266
1700.964286	186.520082	48.367271
1697.559046	196.266300	48.372276
1693.832409	200.755686	48.377281
1690.493962	197.648924	48.382285
1687.461141	193.572752	48.387290
1683.615714	200.219030	48.392295
1680.495027	185.618230	48.397300
1676.580543	186.519126	48.402305
1673.387443	189.902845	48.407309
1669.476802	191.789671	48.412314
1665.929965	188.800377	48.417319
1662.942133	187.862838	48.422324
1659.308314	197.111184	48.427329
1655.570854	189.554499	48.432333
1652.334771	190.538015	48.437338
1648.508034	207.769586	48.442343
1645.268672	188.312803	48.447348
1641.529001	197.127470	48.452353
1637.902728	189.070908	48.457357
1634.619453	187.866729	48.462362
1630.998536	195.541565	48.467367
1627.285340	181.888889	48.472372
1624.253842	186.514676	48.477377
1620.524032	194.592540	48.482381
1617.597149	191.372717	48.487386
1613.674722	189.248192	48.492391
1610.352903	187.427570	48.497396
1606.737676	194.993942	48.502401
1602.974024	186.384020	48.507405
1599.877938	190.686033	48.512410
1595.853455	200.368537	48.517415
1592.498805	188.954410	48.522420
1589.098303	182.335334	48.527425
1585.473262	190.043819	48.532429
1582.275367	188.967442	48.537434
1578.461848	193.182847	48.542439
1575.108692	192.753627	48.547444
1571.947105	191.986765	48.552449
1568.060079	195.536342	48.557453
1564.880134	194.119707	48.562458
1561.031614	188.750850	48.567463
1557.328169	205.874400	48.572468
1553.802187	194.043529	48.577473
1550.269024	195.575709	48.582477
1547.456211	184.351688	48.587482
1543.616484	197.768434	48.592487
1540.080644	182.811617	48.597492
1536.740703	187.279879	48.602497
1533.079635	188.819363	48.607501
1529.911037	180.488353	48.612506
1525.740378	188.864239	48.617511
1522.291685	179.345174	48.622516
1519.077904	188.882672	48.627521
1515.543430	191.407267	48.632525
1512.187933	173.080821	48.637530
1508.132558	194.325789	48.642535
1505.130181	191.871318	48.647540
1501.530154	178.356422	48.652545
1498.212832	179.374624	48.657549
1494.724256	183.511976	48.662554
1491.082966	186.276186	48.667559
1487.666204	183.749231	48.672564
1484.139298	181.819466	48.677569
1480.712082	188.378663	48.682573
1477.189616	178.232806	48.687578
1473.295143	196.676641	48.692583
1469.568770	179.117208	48.697588
1466.111778	187.418356	48.702593
1463.068439	181.540996	48.707597
1459.644272	182.409234	48.712602
1455.879849	187.542973	48.717607
1452.701774	177.118911	48.722612
1449.217293	182.340919	48.727617
1445.607786	186.004381	48.732621
1442.363280	181.443448	48.737626
1438.426479	190.643330	48.742631
1435.003632	184.655279	48.747636
1431.257222	180.678555	48.752641
1427.874686	180.668116	48.757645
1424.541116	181.065628	48.762650
1420.922343	175.377380	48.767655
1417.847204	181.926736	48.772660
1413.850527	178.420085	48.777665
1410.357691	176.642783	48.782669
1406.846175	167.495144	48.787674
1403.007583	178.170005	48.792679
1399.931766	184.917087	48.797684
1396.524739	173.870840	48.802689
1392.669416	177.393963	48.807693
1389.275843	178.239722	48.812698
1385.668248	184.159152	48.817703
1382.772726	173.137013	48.822708
1379.534220	182.705176	48.827713
1375.648109	185.731430	48.832717
1372.124663	175.056119	48.837722
1368.298323	186.167700	48.842727
1364.613409	186.372448	48.847732
1361.531460	172.786643	48.852737
1357.725926	182.519435	48.857741
1354.681590	175.963644	48.862746
1350.944581	182.539594	48.867751
1347.384318	181.337369	48.872756
1343.848256	176.680967	48.877761
1340.255733	180.226939	48.882765
1336.891876	165.288651	48.887770
1333.434776	182.743523	48.892775
1330.343215	183.525651	48.897780
1326.723112	178.403959	48.902785
1322.718834	172.355674	48.907789
1319.275252	179.565902	48.912794
1315.800836	182.531633	48.917799
1312.405110	168.088936	48.922804
1308.789040	177.377502	48.927809
1305.345731	193.917851	48.932813
1301.947312	180.312293	48.937818
1298.572046	176.257220	48.942823
1294.704999	168.822193	48.947828
1291.154170	174.819603	48.952833
1287.776224	171.348034	48.957837
1284.856120	171.614028	48.962842
1280.694783	179.321090	48.967847
1277.608818	177.986254	48.972852
1274.010652	168.532267	48.977857
1270.358411	182.258723	48.982861
1266.904939	181.411929	48.987866
1263.311186	186.931351	48.992871
1259.765058	177.002138	48.997876
1256.160357	183.304721	49.002881
1252.336523	176.830296	49.007885
1249.449762	173.177435	49.012890
1246.186586	179.107061	49.017895
1242.269135	178.583310	49.022900
1238.909978	174.360757	49.027905
1235.439652	188.211598	49.032909
1231.926163	164.279977	49.037914
1228.106333	180.455410	49.042919
1225.080541	178.189026	49.047924
1221.342670	176.256242	49.052929
1217.463768	176.263913	49.057933
1214.085828	160.716468	49.062938
1210.574303	163.664497	49.067943
1207.276246	169.181595	49.072948
1203.598210	178.246424	49.077953
1200.152136	175.297477	49.082957
1197.065835	170.292260	49.087962
1193.335289	184.384464	49.092967
1190.117445	169.530389	49.097972
1186.462095	174.290992	49.102977
1182.569374	182.055576	49.107981
1179.282851	174.337442	49.112986
1175.664017	177.139140	49.117991
1172.275602	176.970468	49.122996
1168.961806	174.408432	49.128001
1164.922843	173.938228	49.133005
1162.149700	183.981528	49.138010
1158.306171	174.581334	49.143015
1155.027505	178.326266	49.148020
1150.858477	182.368435	49.153025
1147.195471	177.170369	49.158029
1144.338880	178.891563	49.163034
1140.487095	185.074180	49.168039
1137.334287	181.582589	49.173044
1133.872139	171.453135	49.178049
1130.017157	163.109188	49.183053
1127.049439	161.770984	49.188058
1122.932914	182.263956	49.193063
1119.879068	177.328297	49.198068
1115.991636	182.086801	49.203073
1112.543438	171.640149	49.208077
1109.557670	159.153631	49.213082
1105.547428	174.959901	49.218087
1102.159083	178.870848	49.223092
1098.991523	173.819703	49.228097
1095.104849	183.747731	49.233101
1091.396848	170.112330	49.238106
1088.219850	166.460401	49.243111
1084.623896	174.386369	49.248116
1081.303219	169.270836	49.253121
1077.353947	176.743709	49.258125
1074.303407	171.519948	49.263130
1070.592324	180.020854	49.268135
1066.980593	174.830847	49.273140
1063.759564	166.570120	49.278145
1059.882273	175.186468	49.283149
1057.013496	167.167502	49.288154
1053.299628	181.638209	49.293159
1049.754700	183.202766	49.298164
1046.040739	167.242979	49.303169
1042.472422	173.746234	49.308173
1039.457659	172.315995	49.313178
1035.513917	175.787506	49.318183
1031.942221	170.761980	49.323188
1028.464282	176.164620	49.328193
1025.212178	177.772100	49.333197
1021.746963	163.933593	49.338202
1017.923230	170.216012	49.343207
1014.584614	165.783409	49.348212
1011.218750	172.822888	49.353217
1007.600007	174.537079	49.358221
1004.250846	164.106409	49.363226
1000.290350	178.227277	49.368231
996.923232	173.185653	49.373236
993.902682	170.679274	49.378241
990.126466	177.984022	49.383245
986.581232	163.991529	49.388250
983.118783	176.368721	49.393255
979.734209	171.017352	49.398260
976.213171	168.750476	49.403265
972.418210	158.161694	49.408269
969.087847	158.840556	49.413274
965.248092	183.156061	49.418279
962.088479	170.884384	49.423284
958.596892	157.962345	49.428289
954.725811	174.543426	49.433293
951.670629	175.687007	49.438298
948.430169	168.049502	49.443303
944.658591	167.781525	49.448308
941.213217	174.733633	49.453313
937.585354	176.191284	49.458317
933.864239	164.588487	49.463322
930.314776	175.830537	49.468327
926.870526	160.363982	49.473332
923.264357	160.177425	49.478337
919.954403	172.716707	49.483341
916.662745	166.469437	49.488346
913.030717	167.848470	49.493351
909.383012	171.316944	49.498356
906.113427	170.493446	49.503361
902.523035	166.567142	49.508365
899.037567	153.870944	49.513370
895.599396	167.642983	49.518375
892.231700	154.359385	49.523380
888.817248	162.442811	49.528385
884.591938	168.486069	49.533389
881.616362	155.534324	49.538394
877.619361	167.967851	49.543399
874.249925	160.170952	49.548404
870.991757	157.574040	49.553409
867.542916	170.342658	49.558413
864.193182	159.335730	49.563418
860.578698	158.339636	49.568423
856.891095	156.097767	49.573428
853.519494	156.841208	49.578433
849.747995	160.000743	49.583437
846.762850	144.285803	49.588442
842.953569	161.052441	49.593447
839.613650	159.497028	49.598452
836.241882	163.242575	49.603457
832.443156	155.203065	49.608461
828.736905	166.525498	49.613466
825.390898	164.001911	49.618471
821.755366	156.585892	49.623476
818.538908	154.585098	49.628481
814.817765	163.535569	49.633485
811.425714	156.888122	49.638490
807.549215	162.613670	49.643495
804.280804	167.446114	49.648500
800.807109	156.400307	49.653505
797.481599	158.797908	49.658509
793.922674	157.922604	49.663514
790.424773	154.312280	49.668519
787.114112	162.612717	49.673524
783.349623	159.551729	49.678529
779.678980	164.735422	49.683533
776.784024	151.799136	49.688538
772.684223	168.617731	49.693543
769.301822	169.696056	49.698548
765.890537	157.151262	49.703553
762.372976	158.319883	49.708557
758.852263	155.862475	49.713562
755.383220	163.696794	49.718567
752.020701	156.671886	49.723572
748.751370	151.293631	49.728577
744.686817	153.264288	49.733581
741.519921	152.963359	49.738586
738.146161	158.557381	49.743591
734.454314	149.934108	49.748596
730.837255	150.290871	49.753601
727.446819	160.912140	49.758605
723.893098	149.001872	49.763610
720.521045	151.238001	49.768615
716.491481	157.693563	49.773620
713.231005	156.596667	49.778625
709.383632	161.279705	49.783629
706.244047	145.283934	49.788634
702.650278	151.364859	49.793639
699.475119	144.507638	49.798644
695.792566	147.597120	49.803649
692.102719	148.371396	49.808653
688.587476	149.230390	49.813658
685.001022	155.529623	49.818663
682.083566	152.091841	49.823668
678.657809	155.702144	49.828673
674.612845	150.352188	49.833677
671.374341	155.343318	49.838682
667.849813	157.580188	49.843687
664.321461	156.410158	49.848692
661.105124	152.496213	49.853697
657.197389	158.413947	49.858701
653.872942	158.183475	49.863706
649.567105	159.816289	49.868711
646.738449	144.365376	49.873716
643.472194	163.298347	49.878721
639.594330	164.669785	49.883725
636.621726	149.178424	49.888730
632.828610	151.221222	49.893735
629.362105	162.190915	49.898740
626.019355	148.777887	49.903745
622.180732	151.928206	49.908749
618.819208	154.332431	49.913754
614.901510	152.067244	49.918759
611.507876	147.021543	49.923764
608.267368	154.410437	49.928769
604.506086	149.420429	49.933773
601.343707	153.174120	49.938778
597.948152	157.856092	49.943783
593.985097	168.875653	49.948788
590.700086	158.519588	49.953793
587.310800	154.498202	49.958797
584.086549	152.210645	49.963802
579.869270	161.183777	49.968807
576.656622	161.094010	49.973812
573.449037	148.610511	49.978817
569.763260	152.582663	49.983821
566.100067	149.081060	49.988826
562.846089	163.557576	49.993831
559.115341	157.896433	49.998836
555.744403	147.533872	50.003841
552.328916	164.031568	50.008845
548.856598	146.773124	50.013850
545.055306	149.178003	50.018855
541.325932	155.323826	50.023860
537.931236	151.171954	50.028865
534.579463	151.523976	50.033869
531.185142	151.813475	50.038874
527.384677	156.756215	50.043879
524.192234	144.518169	50.048884
521.066181	147.553905	50.053889
517.254275	149.641504	50.058893
514.033550	149.268483	50.063898
510.218765	157.875556	50.068903
506.415088	150.901170	50.073908
503.086675	149.809388	50.078913
499.360455	163.602019	50.083917
496.159734	150.737318	50.088922
492.594638	155.990041	50.093927
488.974162	157.723929	50.098932
485.252931	149.823977	50.103937
481.487292	163.319370	50.108941
478.901616	158.200856	50.113946
474.938161	158.374852	50.118951
471.792551	162.725850	50.123956
468.600550	152.329837	50.128961
464.715337	151.493222	50.133965
460.949635	153.574306	50.138970
457.233405	158.725241	50.143975
453.629639	160.141187	50.148980
450.801895	143.817248	50.153985
447.196215	155.548528	50.158989
444.082726	151.744679	50.163994
440.442053	148.266956	50.168999
436.737345	159.225760	50.174004
432.949975	145.211707	50.179009
429.018014	148.139992	50.184013
426.422942	148.828773	50.189018
422.406518	146.615827	50.194023
418.723586	145.035514	50.199028
415.585779	156.576759	50.204033
412.072440	150.176787	50.209037
408.928398	142.821810	50.214042
405.238187	148.378380	50.219047
401.321893	159.930241	50.224052
398.065465	158.423322	50.229057
394.233772	151.318876	50.234061
390.701228	147.436398	50.239066
387.628466	153.486162	50.244071
383.923185	150.677663	50.249076
380.808650	145.055722	50.254081
377.263241	166.207358	50.259085
373.663214	154.385768	50.264090
369.595632	152.713744	50.269095
366.057538	158.002419	50.274100
363.006651	156.243932	50.279105
359.260646	148.170578	50.284109
355.971546	138.575578	50.289114
352.545983	147.602423	50.294119
348.664678	151.677234	50.299124
345.431001	147.801741	50.304129
342.056071	157.798882	50.309133
338.761158	148.377788	50.314138
335.026660	146.574797	50.319143
331.483049	141.592117	50.324148
328.181068	141.905633	50.329153
324.126033	154.882325	50.334157
320.954565	152.107218	50.339162
317.654739	155.066096	50.344167
313.784405	151.714882	50.349172
310.362788	148.982390	50.354177
307.008215	154.159286	50.359181
303.716092	151.456408	50.364186
300.288131	155.756260	50.369191
296.107099	148.593479	50.374196
292.961636	153.480714	50.379201
289.018194	149.642799	50.384205
285.991057	139.264951	50.389210
282.238494	145.267837	50.394215
278.517050	151.643630	50.399220
275.410370	151.417823	50.404225
271.435133	146.884728	50.409229
268.499759	156.783037	50.414234
264.861764	158.859608	50.419239
261.650913	147.920194	50.424244
258.323676	143.695582	50.429249
254.168338	151.986525	50.434253
251.333158	141.165988	50.439258
247.443173	153.359165	50.444263
243.721113	150.760599	50.449268
240.291209	153.089591	50.454273
236.562978	153.672464	50.459277
233.354674	139.516920	50.464282
229.674055	149.671648	50.469287
226.666409	145.124727	50.474292
223.145624	140.476824	50.479297
219.280108	141.533141	50.484301
215.794325	156.433116	50.489306
212.158916	144.435869	50.494311
208.702064	140.531327	50.499316
205.661366	152.368051	50.504321
201.729309	153.201068	50.509325
198.574033	143.239748	50.514330
194.553178	149.860487	50.519335
191.223095	150.157505	50.524340
188.051987	143.830564	50.529345
184.557833	151.727487	50.534349
180.777183	148.906112	50.539354
177.382385	153.241190	50.544359
173.520795	155.350907	50.549364
170.250011	148.197542	50.554369
166.898233	154.397579	50.559373
163.181336	149.025040	50.564378
159.842400	153.579182	50.569383
156.119619	148.231791	50.574388
152.607792	146.288531	50.579393
149.243287	151.653203	50.584397
146.062680	149.376817	50.589402
142.338554	140.602711	50.594407
138.449754	142.578039	50.599412
135.579184	145.084186	50.604417
131.758279	156.417088	50.609421
128.600649	138.059156	50.614426
124.629670	148.708912	50.619431
121.320383	147.715687	50.624436
117.637906	145.446477	50.629441
113.987401	148.447514	50.634445
110.731149	148.357785	50.639450
107.079291	157.470771	50.644455
103.996848	149.221846	50.649460
100.451980	146.974203	50.654465
96.732875	155.933849	50.659469
93.389634	143.700571	50.664474
89.555727	142.889351	50.669479
86.412284	144.209998	50.674484
82.737857	152.957066	50.679489
78.857645	148.932744	50.684493
75.898991	152.224454	50.689498
72.253748	153.721552	50.694503
68.485686	143.428576	50.699508
65.076845	146.027152	50.704513
61.388446	155.368958	50.709517
58.203635	146.428147	50.714522
54.938773	142.605223	50.719527
51.175492	143.397816	50.724532
47.877794	137.238673	50.729537
44.179700	139.764008	50.734541
40.806631	141.509248	50.739546
37.375893	144.703479	50.744551
33.765938	141.952743	50.749556
30.035335	146.228846	50.754561
26.334777	147.318987	50.759565
22.747934	139.326012	50.764570
19.905122	150.048852	50.769575
16.137229	144.453690	50.774580
12.671763	142.022406	50.779585
9.116122	150.820319	50.784589
5.823900	144.794659	50.789594
2.255716	146.275214	50.794599