Thu Jun 16 11:53:13 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.494138	94.561910	0.000000
0.769837	89.917156	0.005005
0.537555	90.216420	0.010010
0.412172	73.693081	0.015014
-0.025752	70.347541	0.020019
-0.210408	73.296658	0.025024
0.170617	64.759793	0.030029
-0.417704	54.950085	0.035034
0.028026	49.720445	0.040038
-0.836006	35.332629	0.045043
-1.155083	27.436218	0.050048
-1.402492	19.966875	0.055053
-2.381400	10.207833	0.060058
-2.379028	8.240633	0.065062
-2.363695	18.284868	0.070067
-2.473184	9.012444	0.075072
-2.510694	-4.459195	0.080077
-3.440880	-0.753732	0.085082
-3.433750	-6.093183	0.090086
-3.440579	7.477507	0.095091
-4.316493	-3.584094	0.100096
-4.354548	1.993759	0.105101
-4.978957	1.491059	0.110106
-4.935225	-15.829131	0.115110
-4.884978	6.211836	0.120115
-5.047312	2.521751	0.125120
-5.703279	-5.468231	0.130125
-6.097078	1.080261	0.135130
-6.210752	1.988934	0.140134
-6.356995	-1.783027	0.145139
-6.305433	0.362380	0.150144
-6.844280	-4.771419	0.155149
-7.568019	-3.733417	0.160154
-7.858296	0.696165	0.165158
-8.205312	2.862553	0.170163
-8.314183	-4.144003	0.175168
-8.165610	-8.324569	0.180173
-8.328170	4.317879	0.185178
-8.220461	-1.246254	0.190182
-8.729508	-1.651312	0.195187
-8.956911	12.054979	0.200192
-9.094667	-0.736161	0.205197
-9.925084	9.462140	0.210202
-9.481527	1.731921	0.215206
-9.871260	-1.703842	0.220211
-10.616993	2.627280	0.225216
-11.053916	10.276471	0.230221
-11.464326	4.289009	0.235226
-11.449767	8.790448	0.240230
-11.680865	0.289666	0.245235
-11.629554	3.770482	0.250240
-11.128509	-2.197327	0.255245
-11.973808	6.267336	0.260250
-12.368063	-4.053660	0.265254
-12.901108	5.707098	0.270259
-12.867698	5.941737	0.275264
-12.877141	-1.780208	0.280269
-13.513300	-6.489403	0.285274
-13.383744	-0.724483	0.290278
-13.991411	1.588172	0.295283
-14.745084	-5.358388	0.300288
-14.764016	1.615499	0.305293
-15.224486	6.917086	0.310298
-15.027569	-4.028807	0.315302
-15.091351	-9.016677	0.320307
-14.887531	1.863162	0.325312
-14.930270	1.754148	0.330317
-16.013213	4.293425	0.335322
-16.186936	5.089496	0.340326
-16.280608	0.955767	0.345331
-16.719915	1.370435	0.350336
-16.618836	-4.065042	0.355341
-17.518975	5.058313	0.360346
-17.727660	0.331154	0.365350
-18.048987	-5.706935	0.370355
-18.119884	3.603750	0.375360
-18.096222	-5.049325	0.380365
-18.217132	-7.550184	0.385370
-18.162401	-1.580131	0.390374
-19.182653	1.901872	0.395379
-19.614361	-1.194296	0.400384
-19.578870	-0.278803	0.405389
-19.719253	4.031104	0.410394
-20.086139	-10.650332	0.415398
-20.189375	-1.888045	0.420403
-20.047933	7.916627	0.425408
-20.589410	-5.312300	0.430413
-21.368709	11.589902	0.435418
-21.068635	0.647281	0.440422
-21.390982	9.909849	0.445427
-21.858694	-2.878058	0.450432
-21.674856	-2.010462	0.455437
-22.048405	-0.515658	0.460442
-22.704945	-3.701735	0.465446
-23.006692	-2.312518	0.470451
-23.136350	3.971735	0.475456
-22.969907	-3.968689	0.480461
-23.378346	-2.350328	0.485466
-23.208165	0.028225	0.490470
-24.085101	6.013344	0.495475
-24.468423	5.062084	0.500480
-24.570363	3.554780	0.505485
-24.931569	8.732925	0.510490
-24.889087	0.972309	0.515494
-24.377652	1.577609	0.520499
-25.471873	0.838638	0.525504
-25.957667	-7.231058	0.530509
-26.156097	8.959651	0.535514
-26.368778	0.073547	0.540518
-26.553633	2.409753	0.545523
-26.709841	6.092377	0.550528
-26.689269	7.234376	0.555533
-26.924420	10.339313	0.560538
-27.707229	-3.198371	0.565542
-27.985858	2.495201	0.570547
-28.118979	4.441959	0.575552
-27.908479	-4.731015	0.580557
-28.264760	-1.571337	0.585562
-28.571598	-3.320119	0.590566
-29.054165	-6.355792	0.595571
-29.422391	6.277138	0.600576
-29.533621	4.145120	0.605581
-29.682203	-5.641522	0.610586
-29.595674	-6.941823	0.615590
-29.745753	-2.952911	0.620595
-30.466569	1.156269	0.625600
-30.739710	1.737034	0.630605
-30.990007	7.341972	0.635610
-30.692144	-4.431530	0.640614
-31.697717	7.930172	0.645619
-32.182996	11.893588	0.650624
-32.494263	3.440782	0.655629
-32.484954	4.387929	0.660634
-32.219734	5.950700	0.665638
-32.294695	7.044166	0.670643
-32.652587	0.193399	0.675648
-32.937406	-1.663496	0.680653
-33.758953	16.685730	0.685658
-34.040707	-2.598824	0.690662
-33.763566	-6.315463	0.695667
-34.095670	1.145336	0.700672
-34.058359	-3.897124	0.705677
-34.938087	2.888531	0.710682
-35.535591	-2.410187	0.715686
-35.765860	0.028428	0.720691
-35.925051	3.128998	0.725696
-35.793184	5.366101	0.730701
-36.121783	5.284895	0.735706
-35.960417	-4.570727	0.740710
-35.998912	6.795956	0.745715
-36.269273	13.086792	0.750720
-36.754673	3.510596	0.755725
-37.334754	6.981714	0.760730
-37.533333	9.992411	0.765734
-37.627893	6.264392	0.770739
-37.890206	7.397304	0.775744
-38.489730	1.339587	0.780749
-39.267692	2.913163	0.785754
-39.179533	0.733199	0.790758
-39.168843	5.021197	0.795763
-39.452465	5.842139	0.800768
-39.358221	2.432643	0.805773
-39.702795	10.584795	0.810778
-39.205361	-0.904817	0.815782
-39.644535	1.634519	0.820787
-40.155404	6.051331	0.825792
-40.206913	2.938796	0.830797
-41.497470	2.264930	0.835802
-41.672649	4.986849	0.840806
-41.825373	10.442185	0.845811
-41.677768	0.013392	0.850816
-42.164682	1.064940	0.855821
-42.675236	17.160244	0.860826
-42.371639	4.021615	0.865830
-42.204222	3.525778	0.870835
-42.749269	6.043249	0.875840
-42.963769	-0.693988	0.880845
-43.437392	-3.155498	0.885850
-43.674509	-0.872313	0.890854
-43.620934	2.041169	0.895859
-44.325967	-0.735275	0.900864
-45.008947	-1.122733	0.905869
-45.644461	-5.987112	0.910874
-44.666461	-7.962534	0.915878
-44.981453	-4.343841	0.920883
-45.247042	7.204110	0.925888
-45.256817	-9.599766	0.930893
-46.362850	4.246491	0.935898
-46.450397	-0.511241	0.940902
-46.996909	1.688809	0.945907
-47.202861	5.979463	0.950912
-46.904929	5.246993	0.955917
-47.244902	-0.580644	0.960922
-47.153858	1.491943	0.965926
-47.108336	7.655596	0.970931
-47.653541	1.485515	0.975936
-48.360450	-8.329898	0.980941
-48.783422	-0.259700	0.985946
-48.830591	-7.705983	0.990950
-48.975232	-10.971720	0.995955
-48.998384	-1.434335	1.000960
-49.949465	-1.479158	1.005965
-50.120179	-2.633460	1.010970
-50.170862	-3.476618	1.015974
-50.447609	-8.569871	1.020979
-50.696294	-4.086394	1.025984
-50.572839	-0.627566	1.030989
-50.893745	3.340155	1.035994
-51.011620	-7.878376	1.040998
-51.860277	-7.767680	1.046003
-52.145739	-3.169212	1.051008
-52.123161	-15.297937	1.056013
-52.158049	-1.400721	1.061018
-52.376829	0.923038	1.066022
-52.365936	2.024709	1.071027
-52.638516	3.087301	1.076032
-53.371284	-1.393917	1.081037
-54.001642	-3.475260	1.086042
-53.631482	7.146041	1.091046
-53.804955	2.828098	1.096051
-54.067780	-4.494646	1.101056
-54.399566	-13.435636	1.106061
-54.970434	-2.099658	1.111066
-55.268478	-7.830635	1.116070
-55.218149	-6.717527	1.121075
-55.454145	-3.550598	1.126080
-55.325529	-11.431294	1.131085
-55.743002	3.992472	1.136090
-56.178893	6.418013	1.141094
-56.208993	4.750956	1.146099
-56.594486	3.364800	1.151104
-57.288183	3.629435	1.156109
-58.181660	7.457679	1.161114
-57.657917	-5.943732	1.166118
-57.679733	-6.737894	1.171123
-58.127457	5.953749	1.176128
-57.862061	-1.758664	1.181133
-58.071894	-12.340873	1.186138
-58.917166	-0.688052	1.191142
-59.465194	-7.635145	1.196147
-59.969481	2.238747	1.201152
-59.685099	3.466975	1.206157
-59.978991	4.240485	1.211162
-59.881543	-3.721484	1.216166
-60.259742	-1.126226	1.221171
-60.267366	6.618835	1.226176
-60.165611	-5.631993	1.231181
-61.268356	-2.693642	1.236186
-61.436400	-4.358716	1.241190
-61.845185	-4.632360	1.246195
-62.054115	-3.152430	1.251200
-61.726083	-4.149628	1.256205
-62.057229	15.683480	1.261210
-62.431128	-1.013068	1.266214
-62.856277	-2.055770	1.271219
-62.804310	9.037886	1.276224
-62.654377	-4.306286	1.281229
-63.686161	-4.356316	1.286234
-64.204711	1.899372	1.291238
-64.825514	-9.165797	1.296243
-64.547553	2.418298	1.301248
-64.025233	1.368963	1.306253
-64.994560	2.892188	1.311258
-65.185186	-2.264132	1.316262
-65.095028	-4.297334	1.321267
-65.353329	2.006696	1.326272
-65.297011	-10.113105	1.331277
-66.443722	4.525448	1.336282
-66.375675	-8.748264	1.341286
-66.332272	-5.773615	1.346291
-66.726217	-3.268292	1.351296
-66.543228	0.409670	1.356301
-67.457190	-3.636630	1.361306
-68.096937	-9.308765	1.366310
-68.066530	2.490167	1.371315
-68.207209	6.988056	1.376320
-68.183883	3.949970	1.381325
-68.641377	12.310593	1.386330
-68.414589	6.188234	1.391334
-69.082650	1.876266	1.396339
-69.486019	3.331804	1.401344
-69.425202	-0.586247	1.406349
-69.822883	4.396081	1.411354
-69.873003	6.544185	1.416358
-70.109599	4.257779	1.421363
-70.812365	12.276459	1.426368
-71.253826	0.828566	1.431373
-71.375806	7.677126	1.436378
-71.664424	10.716219	1.441382
-71.651665	0.041181	1.446387
-71.821651	6.446139	1.451392
-71.638672	-4.250615	1.456397
-71.661713	6.081699	1.461402
-72.120969	-3.326067	1.466406
-72.678854	-4.859233	1.471411
-72.858011	5.855413	1.476416
-73.695547	-2.729319	1.481421
-74.258908	3.721019	1.486426
-74.244218	7.375892	1.491430
-74.127111	-3.540035	1.496435
-74.290149	6.402554	1.501440
-74.741154	7.512985	1.506445
-74.940931	0.900875	1.511450
-74.761871	-10.574191	1.516454
-74.588755	0.700589	1.521459
-75.495159	-0.671393	1.526464
-75.617684	0.615795	1.531469
-76.541854	7.635308	1.536474
-76.372072	5.743830	1.541478
-76.195176	1.700247	1.546483
-77.071910	9.391245	1.551488
-77.561993	1.018510	1.556493
-77.810448	0.421029	1.561498
-77.958637	-1.904650	1.566502
-78.158610	0.733564	1.571507
-78.374761	-3.752431	1.576512
-77.929383	-4.603878	1.581517
-78.184749	11.980982	1.586522
-78.266878	-3.836639	1.591526
-78.836339	0.056834	1.596531
-79.706698	6.099471	1.601536
-79.611199	-2.120449	1.606541
-80.080323	-0.698240	1.611546
-79.745700	4.881550	1.616550
-80.059957	-1.781582	1.621555
-80.756187	5.022682	1.626560
-81.369194	-4.339644	1.631565
-81.879288	8.358855	1.636570
-81.517580	13.477211	1.641574
-81.702351	5.871257	1.646579
-81.747296	6.252913	1.651584
-81.804614	5.571459	1.656589
-82.016280	11.554069	1.661594
-82.040057	5.428234	1.666598
-82.671799	-0.147065	1.671603
-82.974561	2.942704	1.676608
-83.097541	-4.978097	1.681613
-83.457826	1.229139	1.686618
-84.211707	5.933042	1.691622
-84.301421	8.003736	1.696627
-84.611700	7.467674	1.701632
-84.562947	6.803514	1.706637
-84.560614	12.563217	1.711642
-84.846548	3.900047	1.716646
-85.447153	2.610708	1.721651
-85.896969	6.756987	1.726656
-85.925927	8.482319	1.731661
-86.212741	3.713719	1.736666
-86.182544	8.475381	1.741670
-86.307748	5.845405	1.746675
-86.835039	2.761982	1.751680
-87.038462	5.530496	1.756685
-87.963282	10.435394	1.761690
-87.822516	1.363917	1.766694
-87.468348	3.827187	1.771699
-88.117913	8.033806	1.776704
-87.946088	9.099212	1.781709
-88.564651	8.514165	1.786714
-88.972980	4.774177	1.791718
-89.414929	13.950656	1.796723
-89.805634	20.575099	1.801728
-89.709809	11.533931	1.806733
-89.835978	15.163153	1.811738
-89.780714	16.453416	1.816742
-89.964022	1.530821	1.821747
-90.928788	4.355613	1.826752
-90.895294	5.078569	1.831757
-91.217174	2.009636	1.836762
-91.319428	-1.517532	1.841766
-91.093485	-2.252706	1.846771
-92.323468	5.575496	1.851776
-92.412712	4.064517	1.856781
-92.760150	7.131582	1.861786
-92.729569	-6.902469	1.866790
-92.616085	9.059598	1.871795
-93.023257	21.154802	1.876800
-92.755932	2.451040	1.881805
-93.473519	0.473793	1.886810
-94.126053	15.923592	1.891814
-94.256483	10.356692	1.896819
-94.410019	9.445198	1.901824
-94.261819	2.523028	1.906829
-94.607314	5.527422	1.911834
-95.102691	4.613233	1.916838
-95.165549	0.510327	1.921843
-95.717149	5.545519	1.926848
-95.455904	-2.994692	1.931853
-96.073276	4.241464	1.936858
-96.898407	0.361516	1.941862
-97.546367	0.593538	1.946867
-97.521443	6.312312	1.951872
-96.691581	4.034231	1.956877
-97.274854	-2.682992	1.961882
-97.467027	0.312537	1.966886
-97.463603	-1.652663	1.971891
-97.886201	17.218299	1.976896
-98.645018	1.061079	1.981901
-99.123301	0.146433	1.986906
-99.431106	-5.054641	1.991910
-99.316265	-4.255554	1.996915
-99.150420	1.974357	2.006912
-98.976389	11.879604	2.016909
-98.503857	4.285173	2.026906
-97.791471	8.228424	2.036902
-97.786589	6.324415	2.046899
-97.481549	5.528292	2.056896
-96.811536	14.492585	2.066893
-95.897035	2.066368	2.076890
-95.077368	6.644277	2.086886
-95.109154	8.468823	2.096883
-95.158315	3.986568	2.106880
-94.248310	8.623929	2.116877
-93.805031	8.580278	2.126874
-92.578073	10.017951	2.136870
-92.404006	2.921750	2.146867
-92.017804	-2.776764	2.156864
-92.106072	6.243306	2.166861
-91.194125	3.482520	2.176858
-90.575053	7.125003	2.186854
-90.019834	-4.460091	2.196851
-89.036305	5.276547	2.206848
-88.962694	8.658265	2.216845
-88.938463	8.792183	2.226842
-88.356569	7.668587	2.236838
-87.768837	1.221504	2.246835
-86.924338	5.028289	2.256832
-86.354311	6.217298	2.266829
-85.864545	4.877736	2.276826
-85.816213	5.610125	2.286822
-85.200076	4.770145	2.296819
-84.424879	3.217015	2.306816
-84.366944	6.356895	2.316813
-83.667889	7.871444	2.326810
-83.345254	-5.147120	2.336806
-82.111514	3.727015	2.346803
-81.519129	1.141630	2.356800
-81.942377	7.050645	2.366797
-81.536570	4.638288	2.376794
-80.536017	0.815405	2.386790
-80.114049	-0.479861	2.396787
-79.040853	6.909141	2.406784
-78.759370	-3.898067	2.416781
-78.820777	4.088432	2.426778
-78.386619	7.685763	2.436774
-77.248499	-1.047898	2.446771
-76.960542	4.577776	2.456768
-76.990679	0.379282	2.466765
-75.794078	3.203007	2.476762
-75.459011	-8.792429	2.486758
-75.202876	-3.903330	2.496755
-74.062985	3.591011	2.506752
-73.830034	4.575397	2.516749
-73.721233	3.283585	2.526746
-73.482110	2.597730	2.536742
-72.214963	-5.759369	2.546739
-71.820543	-2.400939	2.556736
-71.868171	1.342197	2.566733
-70.742333	-11.754333	2.576730
-70.331883	-9.321398	2.586726
-70.238944	-6.734443	2.596723
-69.912802	-5.190861	2.606720
-68.649601	0.792573	2.616717
-68.704867	-4.050895	2.626714
-67.856061	2.012928	2.636710
-67.297005	-4.396619	2.646707
-67.087307	-0.164579	2.656704
-66.717486	9.445165	2.666701
-65.941094	3.008044	2.676698
-65.506228	-5.617192	2.686694
-64.888900	-1.109064	2.696691
-64.049296	-1.553222	2.706688
-64.008016	1.553010	2.716685
-63.662008	-2.984724	2.726682
-63.358039	4.333554	2.736678
-62.387998	5.303794	2.746675
-62.222295	6.126727	2.756672
-61.078781	4.104524	2.766669
-60.627843	8.586171	2.776666
-60.515472	5.739378	2.786662
-60.496714	-2.149146	2.796659
-59.644665	2.584427	2.806656
-59.216925	5.421231	2.816653
-58.304109	2.252693	2.826650
-57.749910	1.649799	2.836646
-57.818790	-6.252638	2.846643
-57.119196	-0.907567	2.856640
-56.578151	-3.653624	2.866637
-55.954993	8.390303	2.876634
-54.854057	5.341807	2.886630
-54.998160	11.570421	2.896627
-54.603205	10.978682	2.906624
-54.296485	9.674903	2.916621
-53.363042	3.293222	2.926618
-53.038174	6.497251	2.936614
-52.624634	2.393058	2.946611
-51.695582	6.678390	2.956608
-51.301205	9.213704	2.966605
-51.464433	-0.066081	2.976602
-50.318748	4.652699	2.986598
-49.783529	3.404950	2.996595
-49.723684	7.510231	3.006592
-48.849618	-1.513020	3.016589
-48.383067	2.083405	3.026586
-48.031131	5.892181	3.036582
-47.171219	5.846899	3.046579
-46.343587	6.714486	3.056576
-46.823456	3.553906	3.066573
-46.390228	2.925368	3.076570
-45.203567	1.614360	3.086566
-45.084215	5.166867	3.096563
-44.584634	4.817380	3.106560
-43.474845	5.747932	3.116557
-43.390069	7.286018	3.126554
-43.093050	8.869286	3.136550
-42.583578	1.543358	3.146547
-42.020381	8.826949	3.156544
-41.772630	8.256426	3.166541
-40.440305	7.433863	3.176538
-40.242732	6.724747	3.186534
-40.471286	8.718030	3.196531
-39.504378	-0.407540	3.206528
-38.918385	1.475872	3.216525
-38.271036	6.088442	3.226522
-38.121717	10.008445	3.236518
-37.132720	8.399886	3.246515
-36.976943	0.296095	3.256512
-36.819174	8.056475	3.266509
-35.787736	4.562169	3.276506
-35.504860	0.391460	3.286502
-34.616907	3.403506	3.296499
-34.080486	5.209963	3.306496
-33.713713	8.026324	3.316493
-33.695662	3.773930	3.326490
-33.400991	2.219615	3.336486
-32.378840	5.787243	3.346483
-32.179369	-4.503134	3.356480
-31.210870	-0.927035	3.366477
-30.834121	2.466770	3.376474
-30.806834	4.383840	3.386470
-29.733561	2.528384	3.396467
-29.483790	-2.676357	3.406464
-29.058895	9.387501	3.416461
-27.663713	4.695095	3.426458
-27.887033	3.853139	3.436454
-27.766882	0.451550	3.446451
-27.230997	4.063337	3.456448
-26.377758	5.006855	3.466445
-25.954587	1.772108	3.476442
-25.091694	3.779908	3.486438
-24.493128	4.292607	3.496435
-24.342702	6.553824	3.506432
-24.294931	7.521056	3.516429
-23.747910	5.479641	3.526426
-23.098006	5.669689	3.536422
-21.690789	10.982334	3.546419
-21.860315	7.998841	3.556416
-21.305989	14.105022	3.566413
-21.267949	7.094318	3.576410
-19.944841	4.796037	3.586406
-19.556936	4.446979	3.596403
-19.511205	1.787323	3.606400
-19.480650	7.397608	3.616397
-18.095579	3.098733	3.626394
-17.760229	11.007720	3.636390
-17.726566	2.307922	3.646387
-16.432012	3.306775	3.656384
-16.358512	7.864483	3.666381
-16.053442	0.362280	3.676378
-15.296877	4.311825	3.686374
-14.683532	4.248372	3.696371
-14.191523	-0.177126	3.706368
-14.298860	2.788806	3.716365
-13.489718	6.947027	3.726362
-12.746260	-1.395730	3.736358
-12.509968	2.015855	3.746355
-11.731968	1.998041	3.756352
-11.288848	0.281003	3.766349
-11.171615	-3.002852	3.776346
-10.287434	-6.727866	3.786342
-9.955060	1.552970	3.796339
-9.497749	-0.693846	3.806336
-8.352005	3.724349	3.816333
-8.140755	4.757022	3.826330
-7.988781	-2.348123	3.836326
-7.892415	-5.061141	3.846323
-6.974018	-0.423079	3.856320
-6.456831	0.569605	3.866317
-5.590355	11.704325	3.876314
-5.317922	11.427099	3.886310
-5.007531	7.736898	3.896307
-4.484207	18.485701	3.906304
-4.343500	20.294981	3.916301
-3.259869	36.291319	3.926298
-3.072196	31.601789	3.936294
-2.584683	39.640879	3.946291
-2.147530	49.881896	3.956288
-1.961773	63.781530	3.966285
-1.362852	72.042953	3.976282
-0.886309	96.710408	3.986278
-0.141077	119.054447	3.996275
0.000000	126.270001	4.001280
0.185220	127.955710	4.006285
0.203057	139.642592	4.011290
0.526690	149.968133	4.016294
0.578274	156.558513	4.021299
0.435612	150.549731	4.026304
0.582357	158.740239	4.031309
0.544003	179.795747	4.036314
0.984370	178.857519	4.041318
0.945506	184.059601	4.046323
0.980875	190.603249	4.051328
1.162475	184.028063	4.056333
0.888284	196.672839	4.061338
1.095938	187.709169	4.066342
1.223308	191.048025	4.071347
1.109851	187.784192	4.076352
0.909830	189.076211	4.081357
0.844716	186.416440	4.086362
1.165065	179.340446	4.091366
1.039055	183.586864	4.096371
0.831510	189.245475	4.101376
1.368307	190.863719	4.106381
1.226746	192.776478	4.111386
1.169504	194.813321	4.116390
0.810289	181.228548	4.121395
0.839684	187.869370	4.126400
1.533551	190.002579	4.131405
1.074321	190.801248	4.136410
1.586045	184.692697	4.141414
1.435726	183.249207	4.146419
0.980095	167.725647	4.151424
1.163670	162.954132	4.156429
0.889934	183.542547	4.161434
0.996847	183.030364	4.166438
1.179973	191.407548	4.171443
1.403478	191.675591	4.176448
1.440400	189.790362	4.181453
1.053056	188.451449	4.186458
1.409840	189.472691	4.191462
1.430313	188.213872	4.196467
1.197978	190.829745	4.201472
1.374228	192.681401	4.206477
1.268094	197.824658	4.211482
1.230865	177.211627	4.216486
1.157008	197.389973	4.221491
1.004659	185.275785	4.226496
1.183840	184.924895	4.231501
1.188076	199.634171	4.236506
0.960823	186.558643	4.241510
1.233879	193.913215	4.246515
1.042809	194.110469	4.251520
1.545109	203.240525	4.256525
1.225624	212.898445	4.261530
1.409438	214.478738	4.266534
1.589228	220.558533	4.271539
1.655833	216.219300	4.276544
1.753663	219.880119	4.281549
1.513901	221.599666	4.286554
1.923971	207.744890	4.291558
1.463893	211.425295	4.296563
1.345847	209.359682	4.301568
1.613927	210.505190	4.306573
1.193147	217.306445	4.311578
1.371499	219.810257	4.316582
1.248541	228.064314	4.321587
1.092309	226.309457	4.326592
1.804461	216.404500	4.331597
1.513575	225.889200	4.336602
1.688327	224.576667	4.341606
1.686930	218.089421	4.346611
1.616290	217.727233	4.351616
1.916651	223.354702	4.356621
1.595826	221.614517	4.361626
1.858036	226.540447	4.366630
1.833217	226.128955	4.371635
1.738695	218.790617	4.376640
1.685845	226.642514	4.381645
1.437509	229.204213	4.386650
1.606387	226.881048	4.391654
1.489703	230.424306	4.396659
1.302729	234.006508	4.401664
1.811490	242.619360	4.406669
1.607753	256.253590	4.411674
1.633199	253.214313	4.416678
1.835026	247.644600	4.421683
1.950426	255.054457	4.426688
2.195880	258.833939	4.431693
2.331127	260.790244	4.436698
2.462494	245.607725	4.441702
1.984742	238.020170	4.446707
1.693676	238.186694	4.451712
2.100083	227.005057	4.456717
1.800011	241.775514	4.461722
2.012787	255.103944	4.466726
2.060160	257.205685	4.471731
2.060611	252.395051	4.476736
2.029291	238.494804	4.481741
1.932532	243.817262	4.486746
1.966778	250.144082	4.491750
1.983750	259.623505	4.496755
2.006131	268.262292	4.501760
2.573656	270.005395	4.506765
1.970332	255.741013	4.511770
2.013415	233.012403	4.516774
1.977471	247.218025	4.521779
2.071693	263.377512	4.526784
2.268268	259.052600	4.531789
2.150437	266.251409	4.536794
2.208504	263.020874	4.541798
2.226446	259.521921	4.546803
2.119772	263.243577	4.551808
2.177301	268.819839	4.556813
2.506556	270.952345	4.561818
2.367842	256.720887	4.566822
2.074839	248.951065	4.571827
2.123165	267.512686	4.576832
2.606812	252.797476	4.581837
2.208558	243.048183	4.586842
2.610600	253.188979	4.591846
2.059464	241.694792	4.596851
2.149149	234.357278	4.601856
2.284165	251.050736	4.606861
2.342848	256.158193	4.611866
2.596661	251.748747	4.616870
2.423439	269.661136	4.621875
2.268799	258.459332	4.626880
2.460194	257.826933	4.631885
2.072566	269.383413	4.636890
2.283272	250.999750	4.641894
2.517047	264.803686	4.646899
2.209811	262.612568	4.651904
2.385555	256.281010	4.656909
2.090297	259.921068	4.661914
2.390898	261.988954	4.666918
2.445948	257.574766	4.671923
2.101360	255.392289	4.676928
2.148670	256.950454	4.681933
2.009445	267.790295	4.686938
2.463552	265.222284	4.691942
2.424414	288.743650	4.696947
2.693350	292.112209	4.701952
2.472984	282.026874	4.706957
2.326185	301.464576	4.711962
2.403042	286.708236	4.716966
2.679147	288.168020	4.721971
2.290296	291.986037	4.726976
2.334182	294.575518	4.731981
2.291710	292.136624	4.736986
2.663202	282.066441	4.741990
2.649553	289.347093	4.746995
2.364059	303.768528	4.752000
2.864474	290.503107	4.757005
2.518599	299.540759	4.762010
2.920686	292.989566	4.767014
2.917129	284.339640	4.772019
2.930752	293.138722	4.777024
2.635559	293.161301	4.782029
2.417482	290.478252	4.787034
2.724288	293.056247	4.792038
2.868501	308.923296	4.797043
2.669691	299.424542	4.802048
2.989152	300.093645	4.807053
2.513757	313.230118	4.812058
2.813762	323.555636	4.817062
2.985920	325.854891	4.822067
2.946942	323.557281	4.827072
3.205163	314.390436	4.832077
3.061171	314.548835	4.837082
2.679576	294.263067	4.842086
2.833045	310.811181	4.847091
2.721200	322.366619	4.852096
3.201707	309.215459	4.857101
2.819549	330.704556	4.862106
3.214712	311.306549	4.867110
3.195896	320.981046	4.872115
3.098380	313.703237	4.877120
2.867657	303.323142	4.882125
2.819510	307.244581	4.887130
2.974210	318.093401	4.892134
3.036299	329.549167	4.897139
2.832091	332.385251	4.902144
3.051261	324.519603	4.907149
2.885999	333.886631	4.912154
2.428938	335.229032	4.917158
2.821325	328.667785	4.922163
2.889354	329.525633	4.927168
2.883353	333.530877	4.932173
2.888496	334.398428	4.937178
3.033414	335.770192	4.942182
3.026953	365.409604	4.947187
3.299351	360.976634	4.952192
3.535415	354.050634	4.957197
3.193544	370.445477	4.962202
3.584867	352.071898	4.967206
3.388369	339.708676	4.972211
3.038118	333.633204	4.977216
3.363240	331.800959	4.982221
3.354195	331.786016	4.987226
3.451223	321.955119	4.992230
3.261798	326.690237	4.997235
2.981811	321.577475	5.002240
3.434553	328.435188	5.007245
3.110092	339.232489	5.012250
3.610300	341.310215	5.017254
3.438090	341.382515	5.022259
3.200742	332.726902	5.027264
3.668652	333.228424	5.032269
3.258357	342.358138	5.037274
3.576874	342.860672	5.042278
3.303666	331.950992	5.047283
3.339607	350.415611	5.052288
3.785973	355.425886	5.057293
3.546235	342.078026	5.062298
3.644465	332.985063	5.067302
3.588849	331.278087	5.072307
3.262257	334.754048	5.077312
3.267228	334.923247	5.082317
3.173529	347.757828	5.087322
3.415073	339.561433	5.092326
3.445954	358.339141	5.097331
3.420586	358.759499	5.102336
3.654546	352.143230	5.107341
3.337560	368.557932	5.112346
3.150603	366.356689	5.117350
3.456983	361.911001	5.122355
3.381144	367.826220	5.127360
3.686711	357.258609	5.132365
3.430864	371.196236	5.137370
3.505948	365.200813	5.142374
3.525372	367.770276	5.147379
3.267025	373.027438	5.152384
3.712262	380.706832	5.157389
4.029574	398.383221	5.162394
3.680267	397.908835	5.167398
3.959844	391.233414	5.172403
3.836214	397.945096	5.177408
3.558879	376.662438	5.182413
3.576402	388.824094	5.187418
3.839467	389.583123	5.192422
4.243378	389.545318	5.197427
3.809331	385.745153	5.202432
3.906495	386.579643	5.207437
3.587998	380.986163	5.212442
3.638946	390.141396	5.217446
3.539730	389.274369	5.222451
3.601242	397.768644	5.227456
3.962666	395.284692	5.232461
3.718348	399.427104	5.237466
3.867624	401.231054	5.242470
3.991702	399.650942	5.247475
3.863586	398.772906	5.252480
3.698573	389.218295	5.257485
3.799814	394.744563	5.262490
4.187446	388.680018	5.267494
4.130813	397.466007	5.272499
3.854623	397.785259	5.277504
4.122590	387.281260	5.282509
4.268316	397.660341	5.287514
3.705486	400.999849	5.292518
3.761858	401.616837	5.297523
3.999949	402.488120	5.302528
4.117937	385.838395	5.307533
3.942312	400.355020	5.312538
4.210759	397.435675	5.317542
3.790793	397.878526	5.322547
3.955900	404.148760	5.327552
4.389803	412.698509	5.332557
4.317823	420.760548	5.337562
3.912845	394.016664	5.342566
4.029765	407.118374	5.347571
4.227736	412.511361	5.352576
4.512360	416.733391	5.357581
3.980086	422.048563	5.362586
4.252860	422.165023	5.367590
4.479559	425.273630	5.372595
4.407474	426.138952	5.377600
4.408964	402.809245	5.382605
4.186583	403.125129	5.387610
4.058131	397.321967	5.392614
4.267676	403.720509	5.397619
4.202720	429.273137	5.402624
4.257553	421.032773	5.407629
4.248864	426.233304	5.412634
4.316031	420.084969	5.417638
4.168188	418.084235	5.422643
4.136575	410.382221	5.427648
4.288736	421.241990	5.432653
4.565300	423.928298	5.437658
4.525213	422.670787	5.442662
4.496789	425.481981	5.447667
4.162489	426.566638	5.452672
4.456580	419.322424	5.457677
4.476357	429.028199	5.462682
4.315976	421.087502	5.467686
4.006982	417.079612	5.472691
4.262988	423.418492	5.477696
4.407738	416.095370	5.482701
4.484170	429.158803	5.487706
4.534041	415.648579	5.492710
4.755430	419.769677	5.497715
4.307227	421.750995	5.502720
4.517219	428.112872	5.507725
4.341992	443.304573	5.512730
4.822820	441.502324	5.517734
4.758394	452.824102	5.522739
4.794838	451.344395	5.527744
4.859093	423.713246	5.532749
4.841109	423.813728	5.537754
4.492296	429.622250	5.542758
4.926453	422.444269	5.547763
4.700723	424.957080	5.552768
4.685679	424.759431	5.557773
4.551574	419.846576	5.562778
4.809580	420.279794	5.567782
4.666747	428.909964	5.572787
4.443584	428.812808	5.577792
4.508942	424.766038	5.582797
4.637978	448.925389	5.587802
4.452438	454.165810	5.592806
4.576323	452.879324	5.597811
4.589933	460.740682	5.602816
4.762496	451.879340	5.607821
4.622803	453.193770	5.612826
4.663573	457.629744	5.617830
4.608312	464.975168	5.622835
4.627651	462.556813	5.627840
4.571784	453.557119	5.632845
5.001571	472.182623	5.637850
5.214804	472.036829	5.642854
5.186933	467.616060	5.647859
5.292147	462.009652	5.652864
5.282875	454.026306	5.657869
5.084970	446.669131	5.662874
5.037352	458.419853	5.667878
5.202713	451.200054	5.672883
4.832165	451.574856	5.677888
5.404129	459.076288	5.682893
4.785365	458.917240	5.687898
4.796683	456.184612	5.692902
5.124326	458.209284	5.697907
4.904612	463.755270	5.702912
5.114066	453.668739	5.707917
4.699822	457.588070	5.712922
4.788590	452.919641	5.717926
5.094099	453.633479	5.722931
4.994099	479.212008	5.727936
4.948715	477.027211	5.732941
5.123832	485.397199	5.737946
5.302682	487.153554	5.742950
5.391286	481.455765	5.747955
5.083637	480.842195	5.752960
5.142440	479.375267	5.757965
5.165698	493.399868	5.762970
5.111678	486.396651	5.767974
5.166600	474.823837	5.772979
4.777268	485.435437	5.777984
5.549914	482.367345	5.782989
5.153324	487.029705	5.787994
4.865093	475.859783	5.792998
5.192511	485.579078	5.798003
5.321565	486.052845	5.803008
5.054808	474.315654	5.808013
4.862549	490.696161	5.813018
5.060302	493.223054	5.818022
5.132571	503.003171	5.823027
5.482990	514.001807	5.828032
5.638549	525.150546	5.833037
5.705397	520.766890	5.838042
5.488078	505.097351	5.843046
5.541277	498.055001	5.848051
5.216523	490.747673	5.853056
5.335860	482.924587	5.858061
5.456849	516.398314	5.863066
5.462226	512.116569	5.868070
5.792093	521.324937	5.873075
5.330016	516.508179	5.878080
5.537729	518.971474	5.883085
5.418972	524.053293	5.888090
5.432174	519.424167	5.893094
5.638949	514.676630	5.898099
5.564334	528.967236	5.903104
5.815337	516.673957	5.908109
5.242283	519.829409	5.913114
5.612234	526.812276	5.918118
5.774456	511.240425	5.923123
5.618615	516.879859	5.928128
5.615652	519.158262	5.933133
5.656731	522.805742	5.938138
5.742470	516.654891	5.943142
5.619234	513.176646	5.948147
5.581161	520.056559	5.953152
5.807692	530.455920	5.958157
5.682676	516.245931	5.963162
5.950729	518.404075	5.968166
5.984608	509.940315	5.973171
5.784768	518.621984	5.978176
5.928076	514.444316	5.983181
5.899390	511.577901	5.988186
5.950985	519.433997	5.993190
5.980923	499.039007	5.998195
5.566594	497.966458	6.003200
5.679779	508.098432	6.008205
5.614988	508.462564	6.013210
5.644091	515.229659	6.018214
6.002113	520.464134	6.023219
5.807174	525.555780	6.028224
6.095402	510.255031	6.033229
5.742696	520.359429	6.038234
5.424317	523.213625	6.043238
5.776900	518.466162	6.048243
5.562738	517.835859	6.053248
5.873586	523.571116	6.058253
5.643853	532.145856	6.063258
5.753793	522.576801	6.068262
6.145437	513.315967	6.073267
5.730457	506.196487	6.078272
6.191598	514.407347	6.083277
5.914571	521.425010	6.088282
5.846908	518.788096	6.093286
5.958343	513.027132	6.098291
5.596476	525.183717	6.103296
5.680248	519.454847	6.108301
5.584086	520.354836	6.113306
5.645035	524.268168	6.118310
5.853209	514.844582	6.123315
5.513406	525.540860	6.128320
5.511045	519.234977	6.133325
5.869003	528.083839	6.138330
5.847740	522.601998	6.143334
5.914417	517.518207	6.148339
5.506965	521.052263	6.153344
5.413496	524.904789	6.158349
5.515554	523.441659	6.163354
5.616337	524.229190	6.168358
5.632195	530.601290	6.173363
5.774528	543.246675	6.178368
6.306546	548.933850	6.183373
5.883690	540.638584	6.188378
5.724190	531.680240	6.193382
5.733647	532.085672	6.198387
5.819312	544.908534	6.203392
6.123769	534.751003	6.208397
5.742802	526.610027	6.213402
5.696473	529.374772	6.218406
6.067408	536.465115	6.223411
6.038313	523.668208	6.228416
6.032967	522.204970	6.233421
5.862374	523.978628	6.238426
5.829016	518.280460	6.243430
6.059452	518.926106	6.248435
5.827455	526.136109	6.253440
5.932170	520.966415	6.258445
5.690216	524.080076	6.263450
5.751981	525.798662	6.268454
6.181723	522.437197	6.273459
5.849763	518.053249	6.278464
5.871160	525.945416	6.283469
5.740340	518.930901	6.288474
5.844172	524.050520	6.293478
5.900456	513.291367	6.298483
5.223208	523.413785	6.303488
5.699423	520.932251	6.308493
6.021181	523.884979	6.313498
6.040925	527.566175	6.318502
5.970187	515.521505	6.323507
5.995220	529.732603	6.328512
6.037612	519.241916	6.333517
6.089863	514.275050	6.338522
5.656969	528.863316	6.343526
5.960503	521.380915	6.348531
5.817687	532.862803	6.353536
6.193056	522.684287	6.358541
6.206123	523.055481	6.363546
5.868205	520.985416	6.368550
6.007625	517.902884	6.373555
5.966351	512.048374	6.378560
6.032376	497.721099	6.383565
5.769215	498.118111	6.388570
5.184377	483.002314	6.393574
5.735264	501.018864	6.398579
5.613509	517.996753	6.403584
5.935100	516.405002	6.408589
5.920539	523.469267	6.413594
5.707492	526.584268	6.418598
5.858477	516.849498	6.423603
5.430969	524.876227	6.428608
5.883165	523.939181	6.433613
5.753385	519.185107	6.438618
5.875836	523.269802	6.443622
6.170376	523.662160	6.448627
6.051071	532.449803	6.453632
5.847377	521.394525	6.458637
6.164583	524.529927	6.463642
5.895922	523.028516	6.468646
5.587370	494.688934	6.473651
5.798284	509.887230	6.478656
5.827436	522.972861	6.483661
6.056031	522.572560	6.488666
5.891621	509.862448	6.493670
5.664183	506.009760	6.498675
5.631609	512.869917	6.503680
5.980758	503.095601	6.508685
5.746492	523.013694	6.513690
5.656407	522.059419	6.518694
6.214839	516.178513	6.523699
5.687504	517.839560	6.528704
5.834103	513.789799	6.533709
5.634934	513.782894	6.538714
5.533300	514.341252	6.543718
6.127061	519.512402	6.548723
5.816330	517.812245	6.553728
5.949483	522.945763	6.558733
5.952978	526.630039	6.563738
5.779986	512.855755	6.568742
5.963705	507.875354	6.573747
5.561127	498.270255	6.578752
5.971467	511.516635	6.583757
5.885336	523.433693	6.588762
5.828187	499.430828	6.593766
5.471741	504.972788	6.598771
5.461050	528.231931	6.603776
5.525618	515.792670	6.608781
5.722192	530.338180	6.613786
5.760435	526.453715	6.618790
5.959488	531.488936	6.623795
5.598944	543.238457	6.628800
5.714424	525.595032	6.633805
5.936853	531.019634	6.638810
5.861432	530.225324	6.643814
5.976715	525.348667	6.648819
5.608085	526.969775	6.653824
5.768138	524.276682	6.658829
5.849072	524.765900	6.663834
5.891296	537.229723	6.668838
6.146244	520.878444	6.673843
5.722300	528.939115	6.678848
6.270732	528.938200	6.683853
6.082792	528.860084	6.688858
6.050315	530.779127	6.693862
5.982926	522.291054	6.698867
5.740326	514.554104	6.703872
5.365348	509.809674	6.708877
5.734218	525.143382	6.713882
5.683656	535.600575	6.718886
6.119409	529.524569	6.723891
5.614824	527.728391	6.728896
6.153125	527.091633	6.733901
5.939620	532.819527	6.738906
5.669809	529.225902	6.743910
5.785423	523.847227	6.748915
5.765079	530.720170	6.753920
5.809256	529.354704	6.758925
5.804748	538.130582	6.763930
5.644134	537.254850	6.768934
5.542896	532.097779	6.773939
5.583598	530.880577	6.778944
5.961863	526.544408	6.783949
5.599799	526.531470	6.788954
5.664133	538.743223	6.793958
6.023759	529.080318	6.798963
5.761942	531.916487	6.803968
5.879706	536.069146	6.808973
5.939677	525.798513	6.813978
5.861438	532.151732	6.818982
5.868636	524.470871	6.823987
6.084062	530.595118	6.828992
5.873289	523.870347	6.833997
6.123319	530.636752	6.839002
5.698119	527.172691	6.844006
5.920704	535.238202	6.849011
5.839332	529.074513	6.854016
5.956372	526.971192	6.859021
5.835553	526.543394	6.864026
5.797366	530.399216	6.869030
5.763288	521.955658	6.874035
5.513635	532.258696	6.879040
5.733182	532.138101	6.884045
5.686749	523.871304	6.889050
5.758378	535.901110	6.894054
5.887017	530.289425	6.899059
5.647287	538.346493	6.904064
5.933814	527.858865	6.909069
5.584389	540.665821	6.914074
5.808036	528.260047	6.919078
5.923649	523.202795	6.924083
5.597884	541.403628	6.929088
5.960205	535.009158	6.934093
5.734770	536.433757	6.939098
5.316016	531.835955	6.944102
5.891181	540.244537	6.949107
5.957331	532.122111	6.954112
6.123414	519.333994	6.959117
6.157626	522.515372	6.964122
5.700485	533.238742	6.969126
6.071294	522.296097	6.974131
5.448418	523.888780	6.979136
5.809178	531.688562	6.984141
5.805683	528.379848	6.989146
5.413238	527.080519	6.994150
5.877672	530.299620	6.999155
5.898743	527.496604	7.004160
5.948500	527.585990	7.009165
5.918631	535.144493	7.014170
5.628295	519.807146	7.019174
5.797672	519.292029	7.024179
6.065443	534.664750	7.029184
6.204337	525.985130	7.034189
6.532461	524.728323	7.039194
5.955244	533.229274	7.044198
6.265892	519.445599	7.049203
5.793403	514.417662	7.054208
5.695012	496.633413	7.059213
5.860450	496.971732	7.064218
5.535249	498.332311	7.069222
5.565005	505.708397	7.074227
5.770468	531.403163	7.079232
6.063030	534.153046	7.084237
6.155463	525.850769	7.089242
5.613033	519.372006	7.094246
5.665665	509.351310	7.099251
6.267695	523.415749	7.104256
6.050553	517.388942	7.109261
6.163772	507.006624	7.114266
5.577640	509.195530	7.119270
5.839051	501.273976	7.124275
5.883694	491.529863	7.129280
5.541418	489.348548	7.134285
5.676764	494.996581	7.139290
5.434589	498.126354	7.144294
5.753276	517.559325	7.149299
5.651521	538.122950	7.154304
6.011425	532.832057	7.159309
5.873901	537.255392	7.164314
5.980134	530.104028	7.169318
5.940244	520.555196	7.174323
5.415254	527.616701	7.179328
6.068923	523.864349	7.184333
5.880724	530.892495	7.189338
5.965654	533.639891	7.194342
6.013387	508.662021	7.199347
5.435102	509.831990	7.204352
5.568385	522.122804	7.209357
6.143267	521.688659	7.214362
5.730120	525.540147	7.219366
6.017951	522.987438	7.224371
5.825321	524.262971	7.229376
5.900432	511.513769	7.234381
5.732188	509.090100	7.239386
5.582478	515.671280	7.244390
5.952164	509.627609	7.249395
5.708009	520.232803	7.254400
5.816884	522.825986	7.259405
5.816235	535.027066	7.264410
5.703133	537.934160	7.269414
5.695530	527.102091	7.274419
6.058119	532.770693	7.279424
6.045883	526.721170	7.284429
6.051290	522.391766	7.289434
5.635353	517.682219	7.294438
5.676690	504.952908	7.299443
5.776216	522.671843	7.304448
5.766609	515.195812	7.309453
5.942393	523.515297	7.314458
5.718112	527.986509	7.319462
5.582656	528.636880	7.324467
5.730951	533.526487	7.329472
5.589926	524.710415	7.334477
5.662866	524.842536	7.339482
5.691920	536.160075	7.344486
6.070639	526.020564	7.349491
5.751458	532.327868	7.354496
6.219414	531.811454	7.359501
6.136725	520.289168	7.364506
5.737651	526.795343	7.369510
5.798160	522.744713	7.374515
5.765210	519.944212	7.379520
5.742722	517.278129	7.384525
5.762378	523.651867	7.389530
5.930001	520.358087	7.394534
5.776080	515.414736	7.399539
5.989231	532.660001	7.404544
5.969572	527.625595	7.409549
6.113997	530.067880	7.414554
5.864500	518.073467	7.419558
5.754199	502.029998	7.424563
5.418272	508.134460	7.429568
5.665304	517.842988	7.434573
5.797884	522.246544	7.439578
5.746281	537.797143	7.444582
6.228927	525.253367	7.449587
5.825085	524.277739	7.454592
5.720681	529.991647	7.459597
5.895765	524.665397	7.464602
5.639171	531.417854	7.469606
6.019623	534.639293	7.474611
5.861139	531.493914	7.479616
6.063216	521.076776	7.484621
5.692034	518.253246	7.489626
5.585287	522.722397	7.494630
5.826130	523.265595	7.499635
5.484587	527.647466	7.504640
5.848538	523.898400	7.509645
5.793318	531.181696	7.514650
5.512334	532.687592	7.519654
5.609846	529.158854	7.524659
5.747504	523.310089	7.529664
5.609110	529.690119	7.534669
5.920833	536.017471	7.539674
5.558471	527.823993	7.544678
5.786297	525.070075	7.549683
5.768479	533.872321	7.554688
5.917232	521.443709	7.559693
5.992425	527.754898	7.564698
5.672067	527.212189	7.569702
6.064160	517.910632	7.574707
5.764837	535.053931	7.579712
5.935415	530.800424	7.584717
6.070361	534.176974	7.589722
5.861013	536.483271	7.594726
6.150331	527.203033	7.599731
5.828652	534.417600	7.604736
6.035036	537.297053	7.609741
5.766392	524.260436	7.614746
5.869776	530.699364	7.619750
6.226955	529.858426	7.624755
6.023414	531.358825	7.629760
5.692809	509.576310	7.634765
6.018858	511.781400	7.639770
5.518994	516.261450	7.644774
5.817022	510.727441	7.649779
5.882055	523.160450	7.654784
5.890324	525.366262	7.659789
5.761585	530.544048	7.664794
5.712665	534.357348	7.669798
6.102014	532.410186	7.674803
5.610699	538.323492	7.679808
5.940044	523.065954	7.684813
6.064843	529.987423	7.689818
5.721520	520.440394	7.694822
6.161928	497.401558	7.699827
5.454724	494.083849	7.704832
5.628889	508.053239	7.709837
5.739789	518.448319	7.714842
5.794742	527.291119	7.719846
5.593650	528.278691	7.724851
5.558909	530.110699	7.729856
5.491739	541.752839	7.734861
5.964996	534.801668	7.739866
5.710719	531.011024	7.744870
5.699244	534.357213	7.749875
5.721811	541.436069	7.754880
5.664549	537.106954	7.759885
6.070937	522.131964	7.764890
5.941979	530.519670	7.769894
5.606754	527.566678	7.774899
5.646445	533.637391	7.779904
5.840503	534.410495	7.784909
5.799604	533.103583	7.789914
5.904844	521.063666	7.794918
5.881687	533.478405	7.799923
5.791615	541.774748	7.804928
5.601995	524.742606	7.809933
6.149814	526.308751	7.814938
5.730637	548.247137	7.819942
6.081132	536.113996	7.824947
5.838053	531.980149	7.829952
5.791173	538.456146	7.834957
5.824364	530.076939	7.839962
5.453900	535.758063	7.844966
5.867276	525.859466	7.849971
5.529184	537.801106	7.854976
5.620469	544.667446	7.859981
5.973689	539.913261	7.864986
5.597141	539.464584	7.869990
5.928866	535.948243	7.874995
5.845876	540.547942	7.880000
5.699958	535.307983	7.885005
5.729095	526.677282	7.890010
5.703788	527.642612	7.895014
6.000251	529.916128	7.900019
5.664806	528.254979	7.905024
5.636707	525.778452	7.910029
5.757819	537.645883	7.915034
6.030065	538.885931	7.920038
6.033864	521.647502	7.925043
5.816361	533.113911	7.930048
5.838266	534.800215	7.935053
6.054239	518.995030	7.940058
5.751865	535.964015	7.945062
5.911639	530.176410	7.950067
5.673979	526.145851	7.955072
5.533024	530.651734	7.960077
5.853917	532.994910	7.965082
5.718808	535.996009	7.970086
6.000444	527.484883	7.975091
5.559391	543.245858	7.980096
5.683928	531.380820	7.985101
5.615861	540.226199	7.990106
5.725530	555.364220	7.995110
6.010834	565.912434	8.000115
5.854903	562.157448	8.005133
5.882189	555.286282	8.010150
5.911496	553.324696	8.015168
5.967689	559.735974	8.020186
6.068076	553.718101	8.025203
5.752302	547.472116	8.030221
5.812101	539.172749	8.035238
5.683973	533.388670	8.040256
5.848260	546.947816	8.045274
6.011858	556.131416	8.050291
6.121957	546.561001	8.055309
6.015782	528.561261	8.060326
6.140542	532.173391	8.065344
5.667891	546.452135	8.070362
5.553308	541.511210	8.075379
5.684469	537.975145	8.080397
6.006292	550.103335	8.085414
6.010158	544.275397	8.090432
5.722758	545.105543	8.095450
6.130113	555.197088	8.100467
6.260963	552.452049	8.105485
6.046561	545.045258	8.110502
6.122545	531.675077	8.115520
6.107966	544.545229	8.120538
5.986520	537.884536	8.125555
5.990803	548.326880	8.130573
5.856354	549.250132	8.135590
6.205946	544.495338	8.140608
5.661075	543.192893	8.145626
5.943364	531.031669	8.150643
5.978816	540.168340	8.155661
5.819920	541.459039	8.160678
6.070234	536.289937	8.165696
5.869297	543.559180	8.170714
5.888176	546.235957	8.175731
5.856247	534.690025	8.180749
5.726710	546.028611	8.185766
6.355202	548.888938	8.190784
6.160662	551.249777	8.195802
6.262865	550.452477	8.200819
6.031414	544.959722	8.205837
5.574200	546.053512	8.210854
5.873515	547.957127	8.215872
5.775437	569.989210	8.220890
5.803853	562.679656	8.225907
5.756436	573.644727	8.230925
5.898777	577.405998	8.235942
6.278600	569.580097	8.240960
5.930005	574.157287	8.245978
6.242485	563.450100	8.250995
6.204901	574.504571	8.256013
6.389652	573.642949	8.261030
6.671081	562.149324	8.266048
6.176138	567.788771	8.271066
6.175643	553.580007	8.276083
6.053750	551.103361	8.281101
5.869155	546.687187	8.286118
6.201137	557.455029	8.291136
6.329316	562.902049	8.296154
6.235551	558.945566	8.301171
6.199477	539.648863	8.306189
6.015766	535.168484	8.311206
6.357790	537.416837	8.316224
6.266411	541.645078	8.321242
5.999467	530.933688	8.326259
5.942869	538.587554	8.331277
5.898291	543.018156	8.336294
6.208189	539.731137	8.341312
6.378895	560.467767	8.346330
6.163879	559.091916	8.351347
6.060719	553.106992	8.356365
6.374066	561.815252	8.361382
6.317919	541.360686	8.366400
5.903292	549.999517	8.371418
6.395992	563.441821	8.376435
6.167667	542.687723	8.381453
6.167522	549.634871	8.386470
6.403808	552.645329	8.391488
6.379873	546.525982	8.396506
6.390065	530.157161	8.401523
6.341921	533.294327	8.406541
6.373297	540.634408	8.411558
6.352098	531.645524	8.416576
6.162273	537.385097	8.421594
5.982702	533.328355	8.426611
6.200480	534.724784	8.431629
5.778559	549.631335	8.436646
5.999931	546.536662	8.441664
6.457814	562.029571	8.446682
6.540133	561.702389	8.451699
6.531161	571.180996	8.456717
6.157142	563.572963	8.461734
6.141143	566.797521	8.466752
6.500072	573.091073	8.471770
6.309373	572.500706	8.476787
6.511005	565.831877	8.481805
5.824620	561.137377	8.486822
6.269550	560.537716	8.491840
6.322390	569.478264	8.496858
6.252835	575.718537	8.501875
6.621354	574.816608	8.506893
6.303203	574.084147	8.511910
6.706932	556.506994	8.516928
6.509991	567.924635	8.521946
6.140855	568.225881	8.526963
6.067218	563.750035	8.531981
6.413259	560.869256	8.536998
6.654492	562.444057	8.542016
6.210717	574.744742	8.547034
6.540477	566.237690	8.552051
6.937254	563.977925	8.557069
6.365375	563.411089	8.562087
6.378676	537.547345	8.567104
6.453766	531.591327	8.572122
6.191809	545.532067	8.577139
6.282978	556.988979	8.582157
6.087253	562.738294	8.587175
6.283223	565.924675	8.592192
6.425400	573.762201	8.597210
6.648338	564.150888	8.602227
6.852253	564.867959	8.607245
6.404848	578.521724	8.612263
6.653880	569.555963	8.617280
6.455038	568.547244	8.622298
6.466587	567.342471	8.627315
6.484584	570.080310	8.632333
6.178923	567.325039	8.637351
6.394222	568.968582	8.642368
6.588170	573.944104	8.647386
6.624596	571.081032	8.652403
6.817863	565.289291	8.657421
6.282331	573.749633	8.662439
6.467992	567.362814	8.667456
6.738505	574.004177	8.672474
6.484515	564.073434	8.677491
6.515305	561.140444	8.682509
6.525183	573.946748	8.687527
6.433772	568.336472	8.692544
6.095763	568.354679	8.697562
6.642217	569.234489	8.702579
6.391427	562.427970	8.707597
6.426474	564.206003	8.712615
6.432336	567.470837	8.717632
6.260248	564.513019	8.722650
6.318599	562.554111	8.727667
6.796203	561.879183	8.732685
6.336074	568.662148	8.737703
6.370772	563.635142	8.742720
6.386989	576.403794	8.747738
6.674353	591.953351	8.752755
6.895835	594.753808	8.757773
6.695357	587.931879	8.762791
6.627370	571.704941	8.767808
6.645334	577.362858	8.772826
6.760208	581.923585	8.777843
6.958591	565.509455	8.782861
6.608663	570.191666	8.787879
6.575401	555.562812	8.792896
6.512294	565.745691	8.797914
6.577278	578.609119	8.802931
6.988049	577.470234	8.807949
6.737192	567.574200	8.812967
7.022651	559.223852	8.817984
6.631596	561.801678	8.823002
6.886570	563.604279	8.828019
7.076081	563.184890	8.833037
6.869099	561.433871	8.838055
6.708115	571.945463	8.843072
6.941687	563.443877	8.848090
6.358498	560.561180	8.853107
6.508385	557.992189	8.858125
6.559983	578.382165	8.863143
6.707756	558.288384	8.868160
6.586922	564.730001	8.873178
6.382809	569.476383	8.878195
6.806305	572.335658	8.883213
6.627216	594.972676	8.888231
7.108819	592.704497	8.893248
7.144623	591.103078	8.898266
6.880187	589.664637	8.903283
6.457235	575.835446	8.908301
6.442572	584.688654	8.913319
6.483762	592.466713	8.918336
6.924865	590.013928	8.923354
6.339832	602.361005	8.928371
7.057748	603.991260	8.933389
6.757495	600.376111	8.938407
6.836980	600.516722	8.943424
6.685829	603.146426	8.948442
6.391914	603.958856	8.953459
6.780666	599.508830	8.958477
6.698656	606.759729	8.963495
6.920981	606.051411	8.968512
6.912136	595.565772	8.973530
6.474356	598.463269	8.978547
6.804632	601.930255	8.983565
6.731137	618.922263	8.988583
7.032074	626.663713	8.993600
7.019324	627.195869	8.998618
6.774009	638.243286	9.003635
7.079491	624.428389	9.008653
7.084483	642.086941	9.013671
7.215722	632.694734	9.018688
7.161550	614.988502	9.023706
7.025575	601.320481	9.028723
7.123949	598.353977	9.033741
6.916550	598.190888	9.038759
6.734724	590.534253	9.043776
6.699002	600.042294	9.048794
6.591888	617.587678	9.053811
7.032544	612.623661	9.058829
6.823595	624.697034	9.063847
7.179439	625.142004	9.068864
7.282833	628.601026	9.073882
7.073097	631.023235	9.078899
7.392162	615.443661	9.083917
7.119861	604.554204	9.088935
7.010316	602.820929	9.093952
7.072096	602.044181	9.098970
6.328355	598.783956	9.103987
7.032715	608.514708	9.109005
7.077156	617.745589	9.114023
6.878235	623.871560	9.119040
7.292891	615.571765	9.124058
7.156784	629.846634	9.129075
7.267613	628.737533	9.134093
7.400574	631.406100	9.139111
7.207024	610.578362	9.144128
6.919352	602.250770	9.149146
6.660192	617.054913	9.154163
6.990624	605.617220	9.159181
7.513570	623.942661	9.164199
7.345913	624.792582	9.169216
7.235367	620.112035	9.174234
7.012705	609.909702	9.179251
7.038992	609.972410	9.184269
7.349981	612.688112	9.189287
7.128348	620.380609	9.194304
7.084951	612.816910	9.199322
7.080859	613.943282	9.204339
7.168623	618.442765	9.209357
7.305421	625.182905	9.214375
7.224951	611.285865	9.219392
7.295432	619.967083	9.224410
7.206349	626.773581	9.229427
7.316009	616.592787	9.234445
7.082159	621.748939	9.239463
6.984068	626.258276	9.244480
7.374402	614.628528	9.249498
7.459240	624.837185	9.254515
7.435431	617.571366	9.259533
7.163180	605.010585	9.264551
6.780620	632.028923	9.269568
7.172583	618.886215	9.274586
7.088827	627.507608	9.279603
7.240672	623.248368	9.284621
7.268979	621.845192	9.289639
7.287434	623.251541	9.294656
7.613560	618.978754	9.299674
7.226246	631.512722	9.304691
7.399116	626.011871	9.309709
7.201764	636.138158	9.314727
7.161853	638.280976	9.319744
7.343613	618.991573	9.324762
6.956774	634.313287	9.329779
6.871641	629.715232	9.334797
7.159713	627.929432	9.339815
7.190958	634.192828	9.344832
7.140242	626.237595	9.349850
7.334149	631.913494	9.354867
7.563505	629.482509	9.359885
7.047035	627.871782	9.364903
7.206839	644.719479	9.369920
7.737678	648.217098	9.374938
7.578316	649.573225	9.379955
7.629832	638.517359	9.384973
7.693340	624.278370	9.389991
7.293453	632.263761	9.395008
7.459972	624.586740	9.400026
7.480598	630.356713	9.405043
7.773317	618.662304	9.410061
7.834410	618.605995	9.415079
7.429087	631.957834	9.420096
7.574007	622.883878	9.425114
7.425219	629.904632	9.430131
7.535740	621.927874	9.435149
7.612479	623.039807	9.440167
7.099075	635.600323	9.445184
7.479580	621.960788	9.450202
7.521533	634.004613	9.455219
7.245520	626.826325	9.460237
7.461848	638.074759	9.465255
7.290856	633.453399	9.470272
7.487009	625.523401	9.475290
7.316519	633.536126	9.480307
7.258938	630.880173	9.485325
7.431119	640.773285	9.490343
7.353793	659.105958	9.495360
7.517882	661.806386	9.500378
7.843735	679.314142	9.505395
7.697941	665.534914	9.510413
7.795099	652.610646	9.515431
7.497902	638.623340	9.520448
7.575342	640.269007	9.525466
7.418764	658.453883	9.530483
7.414634	661.553395	9.535501
7.433864	653.811938	9.540519
7.548700	660.344052	9.545536
7.891826	652.637340	9.550554
7.731170	667.434110	9.555571
7.347065	655.653037	9.560589
7.358502	643.774626	9.565607
7.390226	662.706382	9.570624
7.671563	663.472955	9.575642
7.342939	662.341414	9.580659
7.118931	667.890857	9.585677
7.665066	651.401849	9.590695
7.312588	654.204961	9.595712
7.593815	660.239003	9.600730
7.343225	686.929685	9.605747
7.696412	683.113341	9.610765
8.215404	681.601026	9.615783
8.002068	688.199882	9.620800
8.178440	673.568156	9.625818
7.828002	665.944366	9.630835
8.007905	664.776515	9.635853
7.888268	659.836879	9.640871
7.821604	662.332576	9.645888
7.918756	662.492902	9.650906
7.616989	665.634515	9.655923
7.929417	664.258777	9.660941
8.201934	659.256009	9.665959
7.920175	666.202316	9.670976
7.974958	660.081330	9.675994
8.024457	659.734969	9.681011
8.134757	664.848826	9.686029
8.014754	656.000780	9.691047
7.588170	664.253342	9.696064
7.666263	666.184379	9.701082
7.687196	663.836248	9.706099
7.965341	669.758817	9.711117
7.835444	669.202976	9.716135
7.868289	669.535019	9.721152
7.863598	655.943955	9.726170
7.876573	661.506388	9.731187
7.659969	673.058039	9.736205
7.867866	669.655394	9.741223
7.492520	662.779373	9.746240
7.781433	664.185904	9.751258
7.507463	660.289385	9.756275
7.428657	660.452909	9.761293
8.013901	662.839496	9.766311
7.715420	670.886087	9.771328
8.090899	676.345222	9.776346
8.210203	678.978758	9.781363
8.144018	671.819307	9.786381
7.902200	659.068843	9.791399
8.127765	659.192596	9.796416
8.367149	660.385112	9.801434
8.026973	662.723293	9.806451
8.094718	668.215075	9.811469
8.307615	661.384631	9.816487
8.140276	676.420459	9.821504
7.749608	669.479264	9.826522
7.733080	664.574841	9.831539
7.998614	668.876589	9.836557
7.937927	657.532227	9.841575
7.541783	662.077347	9.846592
8.036243	663.932787	9.851610
8.278347	664.508933	9.856627
8.016737	657.510498	9.861645
8.122280	661.540023	9.866663
7.821736	670.480772	9.871680
8.158273	675.309658	9.876698
8.148999	679.823522	9.881715
8.376637	686.055960	9.886733
8.147714	663.653010	9.891751
8.050922	671.934130	9.896768
7.703822	666.268848	9.901786
8.298057	674.167225	9.906803
8.045265	702.916552	9.911821
8.642163	692.432496	9.916839
8.230978	679.901796	9.921856
8.253175	676.276148	9.926874
8.218904	670.829784	9.931891
7.884976	664.659079	9.936909
8.015642	665.064112	9.941927
8.142082	687.499034	9.946944
8.080506	687.070653	9.951962
8.196178	692.336260	9.956979
8.014299	700.383474	9.961997
8.311398	698.955258	9.967015
8.330486	700.677982	9.972032
8.120330	684.918525	9.977050
8.185807	692.252748	9.982067
8.205803	696.108070	9.987085
8.356332	688.104099	9.992103
8.576852	704.483750	9.997120
8.188659	700.486533	10.002138
8.253339	690.851403	10.007155
8.085016	697.812731	10.012173
8.557291	692.463814	10.017191
8.390391	699.499894	10.022208
8.523225	691.519609	10.027226
8.303332	693.702806	10.032243
8.229946	692.351067	10.037261
8.475010	689.719879	10.042279
8.385679	693.712240	10.047296
8.317194	697.054533	10.052314
8.649608	696.332250	10.057331
8.133707	688.114163	10.062349
8.665186	668.641830	10.067367
8.445126	678.412324	10.072384
8.353561	665.381072	10.077402
8.331910	658.989604	10.082419
8.416642	672.547740	10.087437
8.382914	667.236102	10.092455
8.148158	663.237353	10.097472
8.141580	672.277132	10.102490
8.521796	677.256938	10.107507
8.192477	700.456429	10.112525
8.371657	695.282398	10.117543
8.410205	690.481442	10.122560
8.374378	703.974210	10.127578
8.447306	691.728387	10.132595
8.438378	698.907127	10.137613
8.391576	696.501693	10.142631
8.203872	702.213816	10.147648
8.341180	701.803641	10.152666
8.478743	690.804764	10.157683
8.177107	698.209202	10.162701
8.360655	688.968127	10.167719
8.420161	695.463740	10.172736
8.503652	707.395267	10.177754
8.747190	692.406527	10.182771
8.441582	695.305817	10.187789
8.727701	697.121197	10.192807
8.377109	705.991513	10.197824
8.337647	698.843574	10.202842
8.736729	705.853041	10.207859
8.388991	723.474622	10.212877
8.637744	708.876364	10.217895
8.883824	722.565724	10.222912
8.405086	717.674490	10.227930
8.672143	718.712172	10.232947
8.453585	720.147758	10.237965
9.068209	720.438571	10.242983
8.842151	700.389554	10.248000
8.522553	696.741070	10.253018
8.749218	696.475349	10.258035
8.283847	693.972289	10.263053
8.306249	702.154512	10.268071
8.866936	726.446188	10.273088
8.763979	721.424953	10.278106
8.743587	724.926496	10.283123
8.434606	737.081338	10.288141
8.361247	727.718062	10.293159
9.007828	724.551610	10.298176
8.740207	726.658955	10.303194
8.967009	731.606860	10.308211
8.785315	723.427305	10.313229
8.664132	720.830952	10.318247
9.166415	725.506405	10.323264
8.662882	738.090959	10.328282
8.980723	717.673548	10.333299
9.087830	732.410288	10.338317
8.863378	715.030349	10.343335
8.861231	701.091649	10.348352
8.732768	704.741237	10.353370
8.755060	710.857846	10.358387
8.898416	722.013697	10.363405
9.163938	725.061181	10.368423
8.889841	708.915296	10.373440
8.532314	704.695337	10.378458
8.854377	707.220287	10.383475
8.853865	718.548503	10.388493
8.571510	722.889539	10.393511
9.037153	724.721113	10.398528
8.663981	731.130203	10.403546
9.168366	722.735322	10.408563
8.548661	733.710550	10.413581
8.879738	716.837113	10.418599
9.217836	715.157581	10.423616
8.874103	729.897969	10.428634
8.946992	718.986812	10.433651
8.878872	722.412105	10.438669
9.088907	719.600516	10.443687
9.182642	723.982826	10.448704
9.210412	724.032398	10.453722
9.210307	713.697074	10.458739
9.024304	711.726668	10.463757
8.882145	694.670193	10.468775
8.810632	712.166601	10.473792
8.825831	719.463386	10.478810
9.130877	716.518699	10.483827
8.987469	725.590961	10.488845
8.933511	719.677550	10.493863
9.027410	722.217280	10.498880
8.724129	732.112857	10.503898
8.823113	722.482666	10.508915
8.757734	722.074200	10.513933
8.643883	733.879533	10.518951
8.830521	727.292132	10.523968
8.714971	724.451292	10.528986
9.319772	730.696897	10.534003
9.057469	741.646034	10.539021
9.091199	720.547661	10.544039
8.980941	730.416555	10.549056
9.164032	746.742998	10.554074
9.520259	741.833141	10.559091
9.064791	745.689111	10.564109
9.112644	734.443563	10.569127
9.234653	736.167882	10.574144
8.686826	733.588105	10.579162
9.618098	741.391162	10.584179
9.293514	754.224548	10.589197
9.532390	736.734558	10.594215
9.217254	732.382020	10.599232
8.998363	733.684126	10.604250
9.252975	726.472521	10.609267
9.185158	735.817380	10.614285
9.241282	746.163022	10.619303
9.498377	732.001664	10.624320
9.015105	738.440859	10.629338
9.492112	739.320643	10.634355
9.274746	746.601553	10.639373
9.661223	736.040255	10.644391
9.544216	722.012173	10.649408
9.548846	722.680311	10.654426
9.394998	713.129105	10.659443
9.345639	707.263354	10.664461
9.284631	716.176058	10.669479
9.178426	707.785651	10.674496
8.778619	709.585769	10.679514
9.319553	718.523484	10.684531
9.222993	742.078491	10.689549
9.361957	740.118343	10.694567
9.450461	738.395229	10.699584
9.452782	756.274783	10.704602
9.521538	746.842055	10.709619
9.598390	752.249897	10.714637
9.284648	751.526244	10.719655
9.461283	741.280865	10.724672
9.189986	740.025497	10.729690
9.363385	743.931647	10.734707
9.378806	744.194341	10.739725
9.348850	746.879321	10.744743
9.829559	740.556250	10.749760
9.201006	744.525354	10.754778
9.395262	738.195301	10.759795
9.669998	747.054212	10.764813
9.498824	738.560767	10.769831
9.547599	736.441541	10.774848
9.655627	745.638571	10.779866
9.650881	731.810192	10.784883
9.466338	749.951873	10.789901
9.590073	748.741930	10.794919
9.510304	741.754835	10.799936
9.336087	738.828037	10.804954
9.108570	745.545774	10.809971
9.336874	746.944025	10.814989
9.282887	753.191146	10.820007
9.373530	752.373113	10.825024
9.380534	754.865802	10.830042
9.551733	746.478144	10.835059
9.535591	758.528911	10.840077
9.593789	772.747398	10.845095
9.949709	760.968533	10.850112
9.607328	758.352340	10.855130
9.729728	758.528767	10.860147
9.612974	749.218703	10.865165
9.622564	750.982464	10.870183
9.931938	747.860317	10.875200
9.758579	751.287853	10.880218
9.422497	752.521844	10.885235
9.919140	760.005965	10.890253
9.656415	757.561514	10.895271
9.913936	754.236658	10.900288
10.235397	748.429765	10.905306
9.878512	750.886249	10.910323
9.748423	749.343226	10.915341
9.886768	746.407777	10.920359
9.985601	741.791588	10.925376
9.834938	742.401843	10.930394
9.681714	733.180772	10.935411
9.855176	744.324972	10.940429
9.955828	734.721067	10.945447
10.173391	734.217428	10.950464
9.943118	739.686452	10.955482
9.652652	735.903740	10.960499
9.899343	737.508065	10.965517
9.736069	732.989611	10.970535
9.884912	725.946637	10.975552
9.730440	736.793814	10.980570
9.893094	744.542824	10.985587
9.932505	732.056000	10.990605
9.827956	738.696141	10.995623
10.122681	740.231812	11.000640
9.741084	744.094960	11.005658
10.056098	739.444030	11.010675
10.107059	740.709513	11.015693
9.630011	737.717625	11.020711
9.962785	731.030989	11.025728
9.753584	748.582666	11.030746
9.639856	741.705100	11.035763
9.985899	743.615779	11.040781
10.097023	764.066624	11.045799
10.253143	761.944908	11.050816
10.060273	756.346017	11.055834
9.571437	747.296518	11.060851
9.879709	762.108781	11.065869
10.043596	778.833140	11.070887
10.292677	774.264735	11.075904
10.060335	775.533346	11.080922
9.864237	779.610093	11.085939
10.414061	771.256880	11.090957
9.991355	790.526144	11.095975
10.299379	779.246425	11.100992
10.385642	768.482796	11.106010
9.937262	763.189953	11.111027
10.393403	762.841141	11.116045
10.077364	751.563016	11.121063
10.132593	754.017526	11.126080
9.959886	742.104620	11.131098
10.111528	760.480957	11.136115
10.439618	775.243412	11.141133
10.055930	766.966236	11.146151
10.045826	769.868370	11.151168
10.310831	777.847482	11.156186
10.296488	776.646775	11.161203
10.166627	773.802288	11.166221
10.198270	778.825856	11.171239
10.393345	768.387093	11.176256
10.155087	770.010058	11.181274
10.138167	781.644222	11.186291
10.689908	774.851710	11.191309
10.360077	770.757150	11.196327
10.292810	779.905034	11.201344
9.959034	769.033491	11.206362
10.502561	775.643306	11.211379
10.111290	765.779303	11.216397
10.270880	782.317699	11.221415
10.486714	783.478691	11.226432
10.692582	783.474426	11.231450
10.416652	788.599308	11.236467
10.306397	776.458281	11.241485
9.946085	789.527576	11.246503
10.466812	779.658493	11.251520
10.434011	778.680085	11.256538
10.748396	780.724814	11.261555
10.371297	786.700506	11.266573
10.633319	779.108690	11.271591
10.448331	769.539666	11.276608
10.439894	780.439202	11.281626
10.544446	783.740125	11.286643
10.529213	765.711695	11.291661
10.517506	778.695129	11.296679
10.469444	775.008838	11.301696
10.618367	773.269339	11.306714
10.267803	761.043455	11.311731
10.296496	763.520654	11.316749
10.187744	768.237857	11.321767
10.355527	766.301973	11.326784
9.935750	775.713876	11.331802
10.044644	770.522503	11.336819
10.201650	763.550197	11.341837
10.056634	782.073400	11.346855
10.533797	788.461260	11.351872
10.643415	792.696799	11.356890
10.571618	800.098139	11.361907
10.897196	797.941232	11.366925
10.848344	803.104463	11.371943
10.725108	786.394594	11.376960
10.643701	785.714517	11.381978
10.734766	797.652833	11.386995
10.931764	785.895489	11.392013
10.465547	771.589799	11.397031
10.438584	768.782629	11.402048
10.822504	788.569548	11.407066
10.622512	798.862882	11.412083
11.050511	798.742595	11.417101
11.082667	801.712933	11.422119
10.901579	774.752978	11.427136
11.025808	770.883620	11.432154
10.624498	778.781150	11.437171
11.008437	772.387656	11.442189
10.634889	775.214150	11.447207
10.599591	766.220768	11.452224
10.740641	774.175981	11.457242
10.451391	766.954155	11.462259
10.835068	762.872074	11.467277
10.721804	775.061814	11.472295
10.444922	763.131763	11.477312
10.624682	782.595101	11.482330
10.843557	797.645357	11.487347
10.831514	795.511376	11.492365
10.964385	793.217645	11.497383
10.698329	796.775350	11.502400
11.343161	799.782013	11.507418
10.882556	803.122803	11.512435
11.256263	810.001104	11.517453
10.703955	800.488727	11.522471
10.641527	797.201481	11.527488
10.839846	803.535054	11.532506
11.072983	806.223901	11.537523
11.227458	794.477513	11.542541
11.055828	805.487385	11.547559
11.054861	800.922900	11.552576
11.375966	792.787556	11.557594
10.980094	799.778859	11.562611
11.095556	774.751509	11.567629
10.732995	779.744866	11.572647
10.859901	788.402487	11.577664
11.146989	798.322864	11.582682
11.137960	796.087124	11.587699
11.049073	797.811171	11.592717
10.953414	796.082271	11.597735
11.479421	794.481106	11.602752
11.379746	803.620878	11.607770
11.256903	788.866081	11.612787
10.814572	786.522749	11.617805
10.819756	783.162534	11.622823
11.413940	790.835728	11.627840
11.508542	785.616108	11.632858
11.184948	782.592750	11.637875
11.300375	772.925564	11.642893
10.901714	775.851761	11.647911
10.813958	771.716311	11.652928
11.107611	799.433177	11.657946
10.954943	809.458708	11.662963
11.331369	792.764469	11.667981
11.190830	807.053224	11.672999
11.104937	801.052065	11.678016
11.385740	800.723469	11.683034
11.354930	801.512505	11.688051
11.233322	796.047365	11.693069
11.034546	799.077417	11.698087
10.725533	794.372538	11.703104
10.665376	791.472147	11.708122
10.795214	801.746305	11.713139
11.054250	820.684187	11.718157
11.262384	830.323890	11.723175
11.254007	827.418774	11.728192
11.318389	824.933738	11.733210
11.228846	830.203389	11.738227
11.125273	829.303196	11.743245
11.561095	830.725616	11.748263
11.372084	841.281877	11.753280
11.532553	830.659556	11.758298
11.631910	835.455162	11.763315
11.603335	823.927746	11.768333
11.172749	830.577522	11.773351
11.444935	831.185803	11.778368
11.597114	816.221290	11.783386
11.409906	837.121359	11.788403
11.631158	820.827073	11.793421
11.624958	831.844855	11.798439
11.784674	828.741619	11.803456
11.911657	828.673339	11.808474
11.639856	819.885217	11.813491
11.475999	817.203102	11.818509
11.544748	815.756224	11.823527
11.557089	816.539704	11.828544
12.012276	815.410487	11.833562
11.496933	807.927439	11.838579
11.380724	808.951805	11.843597
11.399729	809.525856	11.848615
11.722968	816.017004	11.853632
11.636732	822.332857	11.858650
11.777294	837.727135	11.863667
11.533544	821.516481	11.868685
11.498923	825.529161	11.873703
11.621581	827.230061	11.878720
11.990516	820.932415	11.883738
11.414436	840.736046	11.888755
11.476101	821.001559	11.893773
11.813122	831.485547	11.898791
11.524834	842.574752	11.903808
11.525740	829.432428	11.908826
11.458985	824.410490	11.913843
11.213654	826.223177	11.918861
11.518431	825.925947	11.923879
11.276708	835.984318	11.928896
11.610483	841.819922	11.933914
11.679999	860.895944	11.938931
12.075855	860.049805	11.943949
12.199339	848.381221	11.948967
11.725428	846.366857	11.953984
11.945759	829.872357	11.959002
11.701567	834.423710	11.964019
11.879894	839.158147	11.969037
12.158259	847.627712	11.974055
11.840860	835.854764	11.979072
11.876843	826.649309	11.984090
11.581570	828.549565	11.989107
11.921529	843.193414	11.994125
12.062950	857.286042	11.999143
12.139760	857.018710	12.004160
12.129730	846.413630	12.009178
11.679593	834.528687	12.014195
11.756345	845.511220	12.019213
12.356796	849.434013	12.024231
12.232882	846.824903	12.029248
12.456080	828.220386	12.034266
12.079316	831.450101	12.039283
11.947074	818.498261	12.044301
12.203739	809.777508	12.049319
12.068084	816.347542	12.054336
12.073440	816.872875	12.059354
12.113745	821.528362	12.064371
11.998854	817.047647	12.069389
12.303688	821.129894	12.074407
11.978575	821.363054	12.079424
12.255325	823.032388	12.084442
12.199064	816.140961	12.089459
12.284768	812.284061	12.094477
12.245846	818.985818	12.099495
12.018374	827.223472	12.104512
12.318078	816.755873	12.109530
12.212142	824.857617	12.114547
12.354470	825.775788	12.119565
12.267262	811.879976	12.124583
11.807187	824.618312	12.129600
12.149250	823.317766	12.134618
11.965313	818.213936	12.139635
12.049571	817.823841	12.144653
12.489690	833.785916	12.149671
12.025152	842.761836	12.154688
12.069356	843.425113	12.159706
12.246174	858.418612	12.164723
12.586805	864.073892	12.169741
12.499406	852.698668	12.174759
12.320386	857.683172	12.179776
12.600326	852.604818	12.184794
12.612232	835.870692	12.189811
12.263018	835.944479	12.194829
12.331250	815.827981	12.199847
12.119674	831.232816	12.204864
12.599835	845.525115	12.209882
12.827854	844.491497	12.214899
12.546071	839.344490	12.219917
12.379161	829.806686	12.224935
11.777029	828.490354	12.229952
12.398511	845.514390	12.234970
12.334398	858.174035	12.239987
12.490644	848.529185	12.245005
12.778668	853.846173	12.250023
12.743590	847.707882	12.255040
12.480507	851.858993	12.260058
12.065598	852.610737	12.265075
12.661646	853.639525	12.270093
12.700725	851.861979	12.275111
12.492849	855.919830	12.280128
12.364572	848.120778	12.285146
12.551870	846.918627	12.290163
12.470915	844.594292	12.295181
12.462094	845.552990	12.300199
12.461684	845.884235	12.305216
12.631888	838.372019	12.310234
12.724429	851.262710	12.315251
12.704632	839.511038	12.320269
12.492075	834.078234	12.325287
12.370568	849.826109	12.330304
12.600259	839.244596	12.335322
12.433384	853.890534	12.340339
12.742947	850.809470	12.345357
12.806437	848.401138	12.350375
12.703076	856.427389	12.355392
12.859208	866.728342	12.360410
12.766295	858.605291	12.365427
12.271531	868.091539	12.370445
13.164955	865.981603	12.375463
12.902589	877.018428	12.380480
13.023387	877.073982	12.385498
13.061595	853.015983	12.390515
12.523038	849.765881	12.395533
12.682916	863.958793	12.400551
12.946625	878.053963	12.405568
13.532926	861.007802	12.410586
13.260365	850.816113	12.415603
13.124503	849.087553	12.420621
13.150311	836.483525	12.425639
12.954042	839.218836	12.430656
12.946918	836.010517	12.435674
12.994167	840.350453	12.440691
12.498237	839.803528	12.445709
12.914239	828.526988	12.450727
12.935021	839.803359	12.455744
12.901934	841.172290	12.460762
13.036893	834.759494	12.465779
12.808079	840.564469	12.470797
12.868590	840.118960	12.475815
13.206467	850.266662	12.480832
13.377161	848.709448	12.485850
13.199345	836.560644	12.490867
12.825713	835.360557	12.495885
13.204362	828.379935	12.500903
13.030577	833.404208	12.505920
13.105226	839.282042	12.510938
12.887723	846.126588	12.515955
13.143353	852.371788	12.520973
13.514064	855.505636	12.525991
13.212168	863.611049	12.531008
13.435958	855.911558	12.536026
13.055472	842.134151	12.541043
13.200637	847.047463	12.546061
13.210745	833.037241	12.551079
13.025866	844.027681	12.556096
13.418506	870.702231	12.561114
13.471470	865.744929	12.566131
13.234244	866.116096	12.571149
13.274122	852.286139	12.576167
13.296090	851.240321	12.581184
13.441044	859.981302	12.586202
13.381543	845.242947	12.591219
12.967734	866.010455	12.596237
13.177020	860.513539	12.601255
13.141705	869.722818	12.606272
13.156999	878.788822	12.611290
13.456381	864.347965	12.616307
13.205770	870.648096	12.621325
13.707554	867.808441	12.626343
13.608602	879.996096	12.631360
13.521087	860.504772	12.636378
13.778774	855.023576	12.641395
13.371936	869.373617	12.646413
13.786524	859.605079	12.651431
13.693976	862.408375	12.656448
13.985371	848.907457	12.661466
13.788697	830.570219	12.666483
13.371511	827.431535	12.671501
13.552781	825.796507	12.676519
13.280021	823.240733	12.681536
13.713051	829.539564	12.686554
13.666956	825.103668	12.691571
13.402817	834.360088	12.696589
13.852591	839.208791	12.701607
13.605959	834.376880	12.706624
13.644728	835.301832	12.711642
13.750275	828.169429	12.716659
13.618888	814.557832	12.721677
13.943080	824.394452	12.726695
13.704191	827.603055	12.731712
13.787763	823.788523	12.736730
13.285359	829.221462	12.741747
13.661133	848.283269	12.746765
13.931921	834.115324	12.751783
14.057997	836.379530	12.756800
13.542439	835.271881	12.761818
13.774954	828.385473	12.766835
13.620277	844.320187	12.771853
14.218643	851.413007	12.776871
13.678822	850.072698	12.781888
13.650394	838.322748	12.786906
14.119294	839.705162	12.791923
13.713877	850.305064	12.796941
13.925152	836.375649	12.801959
14.141052	842.545635	12.806976
13.778033	839.931657	12.811994
13.863977	820.405618	12.817011
13.317306	843.158066	12.822029
13.968508	852.791874	12.827047
14.034728	863.469230	12.832064
13.784452	868.623849	12.837082
14.012243	865.068493	12.842099
13.850785	866.402843	12.847117
13.993740	860.952512	12.852135
14.140407	864.547028	12.857152
13.888322	868.615337	12.862170
14.157100	862.276363	12.867187
14.037081	870.984480	12.872205
14.042221	860.993402	12.877223
14.181296	865.887553	12.882240
13.769433	863.610716	12.887258
13.850889	863.959233	12.892275
13.844918	862.831138	12.897293
13.996658	861.610850	12.902311
14.091540	869.681400	12.907328
13.802655	858.708494	12.912346
13.791488	863.858434	12.917363
14.170986	880.150692	12.922381
14.020349	875.613084	12.927399
14.222928	877.092160	12.932416
14.277003	879.063505	12.937434
14.422966	879.898318	12.942451
14.113447	892.215742	12.947469
14.606821	881.712256	12.952487
14.514906	885.469212	12.957504
14.151545	877.314972	12.962522
14.375711	871.597818	12.967539
14.516771	893.895120	12.972557
14.481402	874.482449	12.977575
14.320485	871.171018	12.982592
14.138752	864.634986	12.987610
14.495888	863.147237	12.992627
14.319609	868.121450	12.997645
14.433422	874.617119	13.002663
14.568738	881.059641	13.007680
14.171715	873.520006	13.012698
14.512467	875.488160	13.017715
14.354075	884.614755	13.022733
14.443091	884.670443	13.027751
14.567478	885.668045	13.032768
14.439267	883.826032	13.037786
14.643351	873.457448	13.042803
14.385612	893.107770	13.047821
14.887558	882.693500	13.052839
14.831377	879.187725	13.057856
14.358381	877.689645	13.062874
14.920753	873.306403	13.067891
14.229580	871.348899	13.072909
14.506912	870.866377	13.077927
14.561433	878.858381	13.082944
14.706838	879.902893	13.087962
14.554100	879.186085	13.092979
14.738502	886.520330	13.097997
14.507995	877.984260	13.103015
14.397943	884.028337	13.108032
14.356234	878.686160	13.113050
14.955988	865.182981	13.118067
14.820295	883.925886	13.123085
14.592612	882.910989	13.128103
14.778012	870.235785	13.133120
14.847725	887.739561	13.138138
14.685178	873.819732	13.143155
14.614424	879.638456	13.148173
14.471142	882.135140	13.153191
14.626954	884.631010	13.158208
14.346283	878.115161	13.163226
14.235796	896.298900	13.168243
14.837507	911.082793	13.173261
14.612237	915.020820	13.178279
14.733156	909.154997	13.183296
14.769493	915.678248	13.188314
14.955296	906.859231	13.193331
14.734349	911.900572	13.198349
15.274736	912.448200	13.203367
15.348553	906.513405	13.208384
14.842870	911.166644	13.213402
14.961569	905.155449	13.218419
15.049589	907.040789	13.223437
14.933662	907.952833	13.228455
15.330167	906.453948	13.233472
14.811131	918.583026	13.238490
15.224441	907.248519	13.243507
15.063135	907.393203	13.248525
15.026904	906.827385	13.253543
15.154252	896.961238	13.258560
14.848455	909.697177	13.263578
14.917441	903.745960	13.268595
15.146535	908.105758	13.273613
15.290051	912.650041	13.278631
15.651675	912.338200	13.283648
15.053733	908.162637	13.288666
15.251378	895.432642	13.293683
15.223654	918.333652	13.298701
14.875459	912.391048	13.303719
15.056023	899.389415	13.308736
15.164151	909.077283	13.313754
15.776016	912.309258	13.318771
15.296700	906.667999	13.323789
15.157867	902.104814	13.328807
15.132033	904.281852	13.333824
15.277606	902.202601	13.338842
15.236218	908.173737	13.343859
15.490387	913.766961	13.348877
15.604738	917.853847	13.353895
15.774719	911.003126	13.358912
15.525953	910.356900	13.363930
15.136343	899.234597	13.368947
15.647736	903.531898	13.373965
15.451311	904.903914	13.378983
15.665899	899.032752	13.384000
15.682738	910.222736	13.389018
15.367024	906.729632	13.394035
15.448287	909.285849	13.399053
15.260558	910.876171	13.404071
15.331888	906.159182	13.409088
15.533927	924.403296	13.414106
16.027031	922.606805	13.419123
16.049135	914.339248	13.424141
15.463919	910.014757	13.429159
15.383076	905.607115	13.434176
15.569463	903.237904	13.439194
15.514050	904.946787	13.444211
16.056520	918.925469	13.449229
15.724777	910.057552	13.454247
15.857714	897.145371	13.459264
15.330199	911.913844	13.464282
15.708956	907.966176	13.469299
15.859983	908.147616	13.474317
15.670082	920.683638	13.479335
16.032221	917.679585	13.484352
15.751011	906.234793	13.489370
15.723179	906.656874	13.494387
15.791405	905.046817	13.499405
16.060451	912.019217	13.504423
15.895388	910.839175	13.509440
15.585534	901.655793	13.514458
15.695047	914.348789	13.519475
15.880535	934.071068	13.524493
15.512459	926.039212	13.529511
15.933417	922.571683	13.534528
15.845038	941.380940	13.539546
15.516812	930.055986	13.544563
15.967057	935.793456	13.549581
15.562474	935.875803	13.554599
16.065340	928.217543	13.559616
16.087918	931.989147	13.564634
15.727979	933.313889	13.569651
15.937870	925.948293	13.574669
15.811841	926.540116	13.579687
15.904871	920.833496	13.584704
16.234705	945.729709	13.589722
16.150592	950.102505	13.594739
16.203610	941.557531	13.599757
16.169281	936.514059	13.604775
16.444280	924.262605	13.609792
16.030109	929.302720	13.614810
15.983823	924.518269	13.619827
16.589127	931.953815	13.624845
16.345084	942.009097	13.629863
16.010887	935.582959	13.634880
15.841961	935.473930	13.639898
16.356168	960.704003	13.644915
16.341755	954.825100	13.649933
16.324790	956.003616	13.654951
16.925837	946.928784	13.659968
16.312403	933.690486	13.664986
16.072897	922.520924	13.670003
16.350713	927.368550	13.675021
16.282222	954.313706	13.680039
16.634634	950.423127	13.685056
16.256149	954.332556	13.690074
16.354495	955.242159	13.695091
16.823869	959.107819	13.700109
16.350069	947.019649	13.705127
16.506909	939.349483	13.710144
16.357961	949.472209	13.715162
16.681159	953.487886	13.720179
16.609017	950.566124	13.725197
16.278166	947.680816	13.730215
16.587111	950.648250	13.735232
16.585494	960.782949	13.740250
16.515792	953.524851	13.745267
16.850389	947.286854	13.750285
16.788828	950.975731	13.755303
16.679411	936.600295	13.760320
16.562315	944.385599	13.765338
16.483639	959.974075	13.770355
16.949745	946.466637	13.775373
16.437873	968.782101	13.780391
16.936881	962.190215	13.785408
16.918508	960.397550	13.790426
16.830936	935.887654	13.795443
16.633050	939.152484	13.800461
16.669352	938.076245	13.805479
16.857829	944.979313	13.810496
16.921056	956.366450	13.815514
16.725940	957.029721	13.820531
16.657430	946.689996	13.825549
16.668192	959.754107	13.830567
16.979426	952.877958	13.835584
16.923679	952.859064	13.840602
16.664636	951.517317	13.845619
16.963256	954.504762	13.850637
16.665800	959.699584	13.855655
16.440326	952.143369	13.860672
16.833071	947.417240	13.865690
17.098711	952.218863	13.870707
16.860137	962.277683	13.875725
16.962674	962.579026	13.880743
16.834287	946.013410	13.885760
16.828829	955.907150	13.890778
16.816226	956.215613	13.895795
17.123207	961.523307	13.900813
16.906318	957.542784	13.905831
17.163148	963.255053	13.910848
17.304470	965.386172	13.915866
17.231091	968.163686	13.920883
17.311179	956.554543	13.925901
16.815251	960.132559	13.930919
16.971201	970.714467	13.935936
17.434031	980.670477	13.940954
17.108130	984.634599	13.945971
17.297306	990.480182	13.950989
16.911383	986.520991	13.956007
17.183776	979.177614	13.961024
17.287188	980.384655	13.966042
17.291311	990.751158	13.971059
17.395433	976.533079	13.976077
17.300260	981.078252	13.981095
17.552117	976.467113	13.986112
17.296656	970.651951	13.991130
17.355202	985.304554	13.996147
17.571081	974.611471	14.001165
17.762330	976.679332	14.006183
17.628898	976.046813	14.011200
17.487033	967.462881	14.016218
17.360129	989.788564	14.021235
17.680422	984.176033	14.026253
17.419582	980.771071	14.031271
17.695907	974.487191	14.036288
17.683733	980.205935	14.041306
17.538706	986.617283	14.046323
17.804540	982.194940	14.051341
17.307021	984.034755	14.056359
17.736193	972.914469	14.061376
17.640926	972.817573	14.066394
17.821915	980.544877	14.071411
17.544221	985.773148	14.076429
17.542012	981.814612	14.081447
17.520695	976.511346	14.086464
17.425647	980.229283	14.091482
17.460762	977.443996	14.096499
17.820572	979.568337	14.101517
17.565539	968.640142	14.106535
17.743284	975.860098	14.111552
17.831451	971.145916	14.116570
17.553968	969.040128	14.121587
17.911010	968.980672	14.126605
17.677306	978.038778	14.131623
17.530187	972.311500	14.136640
17.703827	974.908849	14.141658
17.521750	974.629681	14.146675
18.103410	984.411458	14.151693
18.171433	995.230019	14.156711
18.083694	993.614827	14.161728
18.099440	974.251938	14.166746
17.811801	973.180123	14.171763
18.006222	976.501566	14.176781
17.827883	970.559113	14.181799
17.653708	984.459272	14.186816
18.132247	1004.421155	14.191834
18.269309	1004.396378	14.196851
18.370996	1000.247077	14.201869
18.219694	997.987386	14.206887
18.018685	984.295722	14.211904
17.733344	989.628684	14.216922
18.124161	998.991596	14.221939
18.605673	991.489169	14.226957
18.321758	1003.589201	14.231975
18.403701	990.447813	14.236992
18.068874	973.488701	14.242010
17.784496	983.740602	14.247027
18.559174	987.143980	14.252045
18.175419	989.464513	14.257063
18.129735	989.825285	14.262080
18.166378	994.292488	14.267098
18.323681	990.388973	14.272115
18.369031	985.490361	14.277133
18.257395	999.032819	14.282151
18.377159	994.282016	14.287168
18.421072	993.474743	14.292186
18.387220	999.189695	14.297203
18.258913	991.429347	14.302221
18.508743	986.381904	14.307239
18.221916	993.009174	14.312256
18.302420	993.208863	14.317274
18.330834	994.517062	14.322291
18.226448	993.247473	14.327309
18.522383	995.522997	14.332327
18.552551	998.319520	14.337344
18.292421	993.199191	14.342362
18.329377	1008.034289	14.347379
18.799912	1017.484612	14.352397
18.941008	1017.088466	14.357415
19.059656	1006.694942	14.362432
18.971028	994.306806	14.367450
18.602728	996.171126	14.372467
19.159513	984.966663	14.377485
18.918434	992.121021	14.382503
19.037217	1002.571520	14.387520
19.312167	983.704173	14.392538
18.678817	996.801148	14.397555
19.176014	994.556415	14.402573
19.289700	987.536057	14.407591
18.868910	989.518185	14.412608
18.970186	978.018595	14.417626
18.310930	972.964034	14.422643
18.715726	985.703648	14.427661
18.977248	995.790851	14.432679
19.037375	986.681883	14.437696
19.255654	983.516191	14.442714
19.149086	992.887784	14.447731
19.402337	982.978339	14.452749
18.918451	971.490233	14.457767
18.750512	968.286418	14.462784
19.042945	969.810093	14.467802
18.903474	979.282964	14.472819
19.083620	973.936762	14.477837
19.238228	990.065059	14.482855
19.032006	981.718583	14.487872
18.873860	995.567392	14.492890
18.911212	989.712199	14.497907
19.149244	977.347739	14.502925
19.089363	985.186097	14.507943
18.941177	988.410250	14.512960
19.186707	982.863116	14.517978
18.908171	987.450598	14.522995
18.772013	982.018401	14.528013
18.947389	983.580512	14.533031
19.061347	985.395741	14.538048
19.329071	990.551791	14.543066
19.253137	1007.725604	14.548083
19.013276	1012.395072	14.553101
19.233778	1017.980613	14.558119
19.426296	1015.257972	14.563136
19.303675	1004.622086	14.568154
19.510242	1018.246895	14.573171
19.410113	1012.758742	14.578189
19.499874	1015.197450	14.583207
19.535307	1025.644812	14.588224
19.275701	1012.711198	14.593242
19.255778	1024.749121	14.598259
19.512150	1016.170992	14.603277
19.347954	1022.283214	14.608295
19.169369	1020.538962	14.613312
19.147058	1019.290841	14.618330
19.333577	1026.614274	14.623347
19.547513	1036.408829	14.628365
19.472079	1037.196886	14.633383
19.885650	1056.419508	14.638400
20.012730	1038.353167	14.643418
20.447907	1032.814236	14.648435
20.167496	1017.596760	14.653453
20.038992	1009.494271	14.658471
19.909456	1009.653781	14.663488
19.879194	1007.697061	14.668506
19.906050	1012.321567	14.673523
20.001946	999.088413	14.678541
19.797659	1006.306862	14.683559
19.938876	1000.306965	14.688576
19.858350	1002.431058	14.693594
19.794019	1011.590994	14.698611
19.622160	1015.920149	14.703629
20.166705	1001.260335	14.708647
19.799384	991.113241	14.713664
19.777978	996.148402	14.718682
19.629926	1014.477048	14.723699
19.748959	997.121704	14.728717
19.808889	1012.231110	14.733735
19.797757	1012.223442	14.738752
20.349674	1021.158045	14.743770
19.921183	1030.659618	14.748787
19.786271	1028.120884	14.753805
20.341493	1022.161205	14.758823
20.087611	1045.202416	14.763840
19.744768	1031.773674	14.768858
20.235611	1042.989047	14.773875
20.028625	1047.598968	14.778893
20.566401	1033.630771	14.783911
20.298996	1047.819181	14.788928
20.606344	1041.100005	14.793946
19.986803	1037.413619	14.798963
20.178972	1040.642550	14.803981
20.311985	1040.377048	14.808999
20.201608	1036.064784	14.814016
20.141253	1043.026337	14.819034
20.033498	1041.438852	14.824051
20.418135	1036.252207	14.829069
20.515300	1030.983270	14.834087
20.317905	1041.471972	14.839104
20.412675	1037.916909	14.844122
20.506957	1036.378306	14.849139
20.678128	1036.978983	14.854157
20.409626	1028.592389	14.859175
20.314361	1047.627284	14.864192
20.430134	1031.066299	14.869210
20.543805	1032.680140	14.874227
20.196568	1051.738966	14.879245
20.661346	1037.389196	14.884263
20.265033	1041.826502	14.889280
20.424779	1061.333454	14.894298
20.589340	1070.355125	14.899315
20.733499	1067.554950	14.904333
20.906795	1059.515337	14.909351
20.837865	1071.496052	14.914368
20.805671	1062.898962	14.919386
20.743496	1069.109185	14.924403
20.506761	1070.315859	14.929421
20.931847	1065.397375	14.934439
20.507088	1067.009170	14.939456
20.900361	1063.411267	14.944474
20.889640	1060.230459	14.949491
20.772829	1065.027417	14.954509
20.998630	1065.776717	14.959527
21.165478	1063.361703	14.964544
20.807075	1063.299237	14.969562
20.706003	1071.039051	14.974579
20.562527	1066.168271	14.979597
21.066269	1058.162422	14.984615
20.906395	1064.740598	14.989632
20.745751	1056.539279	14.994650
20.914504	1054.746186	14.999667
21.095522	1057.012171	15.004685
21.045879	1069.749408	15.009703
21.381903	1083.049980	15.014720
21.537036	1069.044214	15.019738
21.142802	1071.603851	15.024755
21.134436	1064.535727	15.029773
21.517267	1042.954884	15.034791
21.254893	1070.249944	15.039808
21.182429	1065.897948	15.044826
21.300703	1061.813889	15.049843
20.795457	1067.691299	15.054861
21.362069	1072.545076	15.059879
21.389976	1084.189283	15.064896
21.697854	1090.064394	15.069914
21.536373	1076.114092	15.074931
21.327073	1063.496770	15.079949
21.452826	1062.114157	15.084967
21.517353	1068.344675	15.089984
21.385032	1055.181169	15.095002
21.066531	1068.331865	15.100019
21.166407	1091.485522	15.105037
21.492199	1093.179848	15.110055
21.719062	1089.451887	15.115072
21.721075	1087.706714	15.120090
21.636002	1091.936131	15.125107
21.698729	1088.136591	15.130125
22.114560	1086.402942	15.135143
21.672824	1088.856672	15.140160
21.651770	1085.066156	15.145178
21.824754	1086.431364	15.150195
21.666958	1089.859749	15.155213
22.012116	1085.813768	15.160231
21.868884	1061.434797	15.165248
21.509490	1067.017482	15.170266
21.414005	1070.439206	15.175283
21.630320	1077.269636	15.180301
21.853467	1074.069072	15.185319
21.961259	1086.824393	15.190336
21.792954	1087.359441	15.195354
21.951270	1085.115193	15.200371
21.724448	1093.623800	15.205389
21.804301	1085.563696	15.210407
21.655308	1088.412576	15.215424
21.702147	1096.566664	15.220442
21.749949	1090.186272	15.225459
21.649700	1083.283198	15.230477
21.822558	1087.710402	15.235495
21.624150	1094.309424	15.240512
21.934031	1104.804482	15.245530
22.135684	1108.975598	15.250547
22.050556	1111.054707	15.255565
22.314568	1102.068939	15.260583
22.425873	1116.518199	15.265600
22.279370	1112.722624	15.270618
22.361758	1104.967058	15.275635
22.238161	1106.969664	15.280653
22.586221	1107.458350	15.285671
22.307873	1106.969044	15.290688
22.442714	1106.807059	15.295706
22.394634	1093.574589	15.300723
22.108733	1102.616201	15.305741
22.495628	1105.178824	15.310759
22.535426	1105.503921	15.315776
22.492859	1101.779150	15.320794
22.405375	1096.584299	15.325811
22.405655	1109.584041	15.330829
22.445874	1109.909069	15.335847
22.424933	1104.353279	15.340864
22.452960	1106.247967	15.345882
22.644078	1110.436176	15.350899
22.728762	1110.684380	15.355917
22.811605	1109.256992	15.360935
22.854487	1110.650690	15.365952
22.310519	1098.967825	15.370970
22.538698	1100.262999	15.375987
22.919866	1113.417874	15.381005
22.650251	1097.145367	15.386023
22.848566	1108.288678	15.391040
22.495939	1113.501623	15.396058
22.644820	1101.635178	15.401075
22.631864	1112.683900	15.406093
22.718491	1110.626466	15.411111
22.710854	1111.064109	15.416128
22.545383	1112.726450	15.421146
22.602819	1109.290414	15.426163
22.614678	1113.357289	15.431181
23.031524	1109.132259	15.436199
22.824362	1108.580410	15.441216
22.636746	1110.945701	15.446234
23.040505	1116.662482	15.451251
22.905447	1147.510148	15.456269
23.062549	1152.209810	15.461287
22.871607	1141.114923	15.466304
23.031125	1128.759379	15.471322
23.282676	1138.975370	15.476339
22.913450	1147.013626	15.481357
23.192899	1138.560236	15.486375
23.289885	1141.218403	15.491392
23.195264	1136.949563	15.496410
23.324191	1133.310598	15.501427
22.973232	1138.546894	15.506445
23.095931	1137.008998	15.511463
23.471021	1130.033650	15.516480
23.457267	1134.317522	15.521498
23.609515	1136.167085	15.526515
23.421773	1130.749067	15.531533
23.549832	1128.105945	15.536551
23.570010	1125.948288	15.541568
23.238137	1128.098090	15.546586
23.334725	1130.083207	15.551603
23.560275	1130.900552	15.556621
23.701994	1125.102556	15.561639
23.377366	1129.668863	15.566656
23.435858	1121.444286	15.571674
23.419761	1119.073568	15.576691
23.310221	1125.289870	15.581709
23.817639	1134.690084	15.586727
23.474620	1125.981358	15.591744
23.024401	1132.032739	15.596762
23.367225	1135.673532	15.601779
23.173546	1137.656035	15.606797
23.567079	1129.208399	15.611815
23.645240	1130.092220	15.616832
23.562643	1150.978380	15.621850
23.783038	1152.589556	15.626867
23.928396	1160.732121	15.631885
23.855729	1153.817176	15.636903
23.877921	1161.682704	15.641920
23.545608	1156.526126	15.646938
23.972646	1159.505479	15.651955
23.760435	1157.353549	15.656973
23.885669	1151.975127	15.661991
23.919320	1162.253515	15.667008
23.870669	1156.902055	15.672026
24.143275	1155.947747	15.677043
23.746574	1161.599613	15.682061
23.817236	1154.390161	15.687079
23.942506	1153.740862	15.692096
23.826623	1155.216500	15.697114
23.941154	1151.384864	15.702131
24.280363	1144.559313	15.707149
24.266920	1157.301957	15.712167
24.188078	1160.698907	15.717184
24.047691	1156.883613	15.722202
24.243737	1144.995563	15.727219
24.297278	1157.349249	15.732237
23.879937	1164.931567	15.737255
24.237075	1166.978535	15.742272
24.211693	1182.185165	15.747290
24.360733	1183.793374	15.752307
24.505781	1175.184251	15.757325
24.634328	1177.544935	15.762343
24.979727	1174.738351	15.767360
24.797663	1168.368358	15.772378
24.704678	1145.992032	15.777395
24.599440	1134.525173	15.782413
24.515960	1146.544467	15.787431
24.709757	1125.309163	15.792448
24.263131	1130.377045	15.797466
24.676231	1134.065860	15.802483
24.737885	1138.273109	15.807501
24.366216	1136.612022	15.812519
24.569007	1153.415681	15.817536
24.883204	1171.411771	15.822554
24.787272	1158.284577	15.827571
25.069128	1164.686567	15.832589
24.651383	1152.785394	15.837607
24.931596	1130.740266	15.842624
24.394858	1140.623611	15.847642
24.756706	1142.554069	15.852659
24.936735	1170.244131	15.857677
25.204355	1179.081738	15.862695
25.260392	1165.008514	15.867712
24.734537	1152.023029	15.872730
24.990083	1135.777063	15.877747
24.730726	1143.503510	15.882765
24.880089	1157.380276	15.887783
24.860627	1177.967702	15.892800
25.117882	1171.891978	15.897818
25.423088	1160.138214	15.902835
25.169773	1167.320261	15.907853
24.912269	1170.644393	15.912871
25.244931	1163.535317	15.917888
24.679981	1176.614154	15.922906
25.227773	1159.930563	15.927923
25.273131	1163.313878	15.932941
25.018204	1178.042578	15.937959
25.352756	1163.605076	15.942976
25.407629	1153.209592	15.947994
25.569054	1163.801653	15.953011
25.504215	1165.754208	15.958029
25.253032	1161.732062	15.963047
25.530531	1152.412596	15.968064
25.559822	1166.106884	15.973082
25.519326	1160.838509	15.978099
25.657044	1156.320871	15.983117
25.315845	1165.258881	15.988135
25.758865	1174.647915	15.993152
25.428625	1169.533503	15.998170
25.367815	1159.321671	16.003187
25.796186	1167.304695	16.008205
25.220647	1167.721442	16.013223
25.402407	1151.968479	16.018240
25.251250	1174.355712	16.023258
25.767587	1167.539653	16.028275
25.532616	1157.451273	16.033293
25.268391	1155.808446	16.038311
25.641883	1169.281710	16.043328
25.691320	1186.418571	16.048346
25.797065	1192.551891	16.053363
26.258892	1194.814201	16.058381
26.079369	1190.014584	16.063399
26.059995	1184.634658	16.068416
26.168576	1179.934260	16.073434
25.933104	1163.746182	16.078451
26.223468	1162.045560	16.083469
25.623778	1157.751141	16.088487
25.727759	1168.629029	16.093504
25.616099	1179.809839	16.098522
26.053242	1189.651747	16.103539
26.048390	1186.668827	16.108557
25.667553	1195.066055	16.113575
26.358375	1177.752609	16.118592
26.243095	1196.649091	16.123610
26.119001	1192.384122	16.128627
26.301633	1184.559006	16.133645
26.049472	1195.571542	16.138663
26.337608	1190.867252	16.143680
25.782912	1195.102760	16.148698
25.898426	1189.144728	16.153715
26.147816	1209.817471	16.158733
26.303222	1209.278723	16.163751
26.620721	1213.029214	16.168768
26.782655	1214.559128	16.173786
26.366010	1221.235797	16.178803
26.486957	1215.499458	16.183821
26.268897	1214.550850	16.188839
26.539725	1208.803129	16.193856
26.452355	1223.843301	16.198874
26.587273	1223.568722	16.203891
26.798030	1217.464252	16.208909
26.252318	1210.954762	16.213927
26.891769	1211.360659	16.218944
26.641926	1223.324448	16.223962
26.583256	1221.192601	16.228979
26.761324	1216.456697	16.233997
26.476360	1217.529446	16.239015
26.511071	1224.127789	16.244032
26.780580	1212.883346	16.249050
26.780481	1221.515850	16.254067
26.842323	1218.581145	16.259085
26.684465	1219.227444	16.264103
27.038312	1211.120913	16.269120
26.981741	1220.798209	16.274138
26.558558	1216.810376	16.279155
27.009292	1216.429287	16.284173
26.944529	1222.412084	16.289191
27.284247	1245.761243	16.294208
27.144239	1231.798492	16.299226
27.279159	1212.386677	16.304243
27.468295	1208.742665	16.309261
27.170646	1220.581303	16.314279
26.790286	1211.030609	16.319296
26.978045	1215.212513	16.324314
27.101703	1232.159432	16.329331
27.504096	1233.582496	16.334349
27.374655	1243.317707	16.339367
27.476057	1229.241848	16.344384
27.638757	1230.570094	16.349402
27.463596	1220.912662	16.354419
27.485560	1224.341188	16.359437
27.286273	1213.445036	16.364455
27.610058	1209.905327	16.369472
27.674436	1221.310185	16.374490
27.021385	1204.887380	16.379507
27.314151	1214.379404	16.384525
27.355247	1231.079772	16.389543
27.743225	1238.398161	16.394560
27.281932	1237.610395	16.399578
27.719731	1235.941297	16.404595
27.872699	1229.529298	16.409613
27.568631	1239.133547	16.414631
27.631963	1237.768811	16.419648
27.634036	1240.079746	16.424666
27.585271	1228.681228	16.429683
27.356323	1232.266358	16.434701
27.767367	1239.719693	16.439719
27.634563	1229.193977	16.444736
27.752644	1235.614796	16.449754
27.726071	1260.916918	16.454771
28.005693	1247.748449	16.459789
28.100675	1257.592425	16.464807
28.373023	1257.838552	16.469824
28.267420	1240.064617	16.474842
28.285921	1238.375453	16.479859
28.136478	1224.034999	16.484877
27.922243	1225.260994	16.489895
28.219056	1220.332463	16.494912
28.062036	1218.430023	16.499930
28.059796	1220.259267	16.504947
28.388163	1236.570886	16.509965
28.377524	1252.082383	16.514983
28.451378	1227.440539	16.520000
28.192861	1217.620927	16.525018
28.146092	1226.160572	16.530035
28.331965	1225.228269	16.535053
28.142525	1251.717338	16.540071
28.493418	1254.470552	16.545088
28.764221	1251.315906	16.550106
28.556438	1250.420510	16.555123
28.815789	1242.132760	16.560141
28.509920	1227.353660	16.565159
28.349273	1213.723810	16.570176
28.323744	1220.857809	16.575194
28.310939	1236.781982	16.580211
28.701981	1239.301233	16.585229
28.579812	1252.208357	16.590247
28.613099	1247.411343	16.595264
28.591961	1242.471184	16.600282
28.469214	1254.501578	16.605299
28.854934	1253.444728	16.610317
28.316835	1250.221820	16.615335
28.475447	1255.989990	16.620352
28.895928	1251.062859	16.625370
28.649452	1247.874227	16.630387
28.455764	1252.253407	16.635405
28.760513	1267.034759	16.640423
29.125760	1272.122436	16.645440
29.070799	1274.893911	16.650458
28.965383	1282.191115	16.655475
29.360586	1262.303813	16.660493
29.085537	1277.210117	16.665511
29.260874	1282.516945	16.670528
29.403860	1270.818837	16.675546
29.568056	1255.051744	16.680563
29.000341	1246.306471	16.685581
28.919496	1246.196660	16.690599
29.204818	1258.838647	16.695616
29.674100	1264.651530	16.700634
29.582867	1259.869776	16.705651
29.326184	1240.729494	16.710669
28.953042	1246.546958	16.715687
29.250910	1258.839487	16.720704
29.516750	1255.073752	16.725722
29.484292	1280.999024	16.730739
29.305232	1268.475930	16.735757
29.432339	1273.023918	16.740775
29.152857	1270.567391	16.745792
29.824449	1268.377645	16.750810
29.606584	1273.506377	16.755827
29.482530	1268.378328	16.760845
29.427731	1279.038084	16.765863
29.246591	1262.808449	16.770880
29.531703	1264.926772	16.775898
29.410196	1270.770171	16.780915
29.637755	1264.887083	16.785933
29.813765	1292.776621	16.790951
29.842311	1300.266032	16.795968
30.326500	1296.411457	16.800986
30.098167	1285.504898	16.806003
30.321267	1268.200544	16.811021
30.006398	1263.543133	16.816039
29.974054	1263.622126	16.821056
30.110288	1257.371122	16.826074
30.078998	1257.606806	16.831091
30.130841	1250.689349	16.836109
29.962644	1250.409751	16.841127
30.323714	1250.984271	16.846144
30.204782	1259.305187	16.851162
30.215533	1269.996618	16.856179
30.291560	1257.691967	16.861197
30.047159	1259.649605	16.866215
29.958946	1260.975034	16.871232
30.336668	1257.050083	16.876250
30.420740	1260.782280	16.881267
30.168386	1266.975594	16.886285
30.179810	1268.354823	16.891303
30.217025	1283.120962	16.896320
30.492139	1287.473264	16.901338
30.727253	1287.847376	16.906355
30.786919	1293.315623	16.911373
30.612147	1289.442798	16.916391
30.555069	1286.809183	16.921408
30.692524	1277.434647	16.926426
30.635435	1281.036854	16.931443
30.773247	1278.138592	16.936461
30.850494	1266.695800	16.941479
30.452060	1256.770565	16.946496
30.769625	1270.319096	16.951514
30.662047	1279.136689	16.956531
30.722825	1288.183905	16.961549
30.813742	1289.518115	16.966567
30.789468	1290.127777	16.971584
30.885508	1284.337663	16.976602
30.675099	1295.549440	16.981619
30.790681	1279.288270	16.986637
30.753861	1286.945933	16.991655
30.658639	1297.773183	16.996672
30.998882	1283.819591	17.001690
30.648473	1294.576823	17.006707
30.995077	1285.178151	17.011725
30.882147	1281.853485	17.016743
30.825288	1298.981466	17.021760
31.211429	1313.721072	17.026778
30.893196	1325.640344	17.031795
31.157074	1320.546581	17.036813
31.310342	1313.046872	17.041831
31.293679	1324.130802	17.046848
31.463408	1312.740596	17.051866
31.216902	1318.362974	17.056883
31.056952	1311.966436	17.061901
31.140646	1313.401432	17.066919
31.274762	1320.886004	17.071936
31.228602	1320.369146	17.076954
31.638554	1333.956001	17.081971
31.614826	1328.952669	17.086989
31.915179	1340.517211	17.092007
31.679602	1334.364621	17.097024
31.950523	1312.062345	17.102042
31.736380	1315.214801	17.107059
31.299903	1327.204591	17.112077
31.914841	1325.229680	17.117095
32.092806	1328.154572	17.122112
31.787075	1322.404070	17.127130
31.735357	1314.201539	17.132147
31.808283	1327.488233	17.137165
32.224844	1335.209361	17.142183
31.483616	1340.253565	17.147200
32.043709	1337.496893	17.152218
31.947359	1334.723523	17.157235
32.126280	1336.038667	17.162253
32.077367	1336.822455	17.167271
32.199401	1340.607247	17.172288
32.469680	1331.558903	17.177306
32.088414	1341.223406	17.182323
32.383983	1336.594407	17.187341
32.613202	1336.494764	17.192359
32.305061	1333.120272	17.197376
32.070235	1317.695586	17.202394
32.173179	1324.251599	17.207411
32.048260	1338.770022	17.212429
32.369638	1340.965224	17.217447
32.144844	1342.553547	17.222464
32.202512	1352.006371	17.227482
32.057784	1343.913864	17.232499
32.008692	1333.325826	17.237517
32.426047	1347.660369	17.242535
31.936609	1347.556276	17.247552
32.395664	1357.554490	17.252570
32.573708	1363.069922	17.257587
32.468369	1378.859163	17.262605
32.864347	1356.214356	17.267623
32.556493	1368.191386	17.272640
33.025190	1369.323628	17.277658
32.851466	1364.177578	17.282675
32.842506	1367.257364	17.287693
33.236101	1360.822866	17.292711
33.042623	1358.976032	17.297728
33.277760	1353.896258	17.302746
32.774074	1368.998087	17.307763
32.942437	1355.533589	17.312781
33.034585	1356.919365	17.317799
32.884953	1371.246066	17.322816
32.993749	1352.989198	17.327834
33.158461	1356.858070	17.332851
33.200868	1364.875455	17.337869
33.332330	1358.683262	17.342887
33.183961	1358.178766	17.347904
33.315629	1345.773328	17.352922
33.431853	1351.984299	17.357939
33.306063	1362.400175	17.362957
33.522802	1350.910651	17.367975
33.133244	1358.942142	17.372992
33.486479	1351.783721	17.378010
33.098635	1355.465009	17.383027
33.236858	1350.669517	17.388045
33.058112	1354.408954	17.393063
33.392491	1362.582782	17.398080
33.544995	1355.605933	17.403098
33.294563	1349.949613	17.408115
32.844424	1372.904769	17.413133
32.972524	1377.547099	17.418151
33.501554	1386.779159	17.423168
33.749499	1380.475201	17.428186
33.897233	1377.537688	17.433203
33.889234	1365.605246	17.438221
34.493902	1378.727353	17.443239
33.905455	1377.447481	17.448256
33.997263	1375.202964	17.453274
34.103136	1384.499242	17.458291
33.860450	1383.052209	17.463309
33.843764	1371.365649	17.468327
33.968485	1381.288045	17.473344
33.874142	1380.576226	17.478362
34.121411	1379.283821	17.483379
33.894297	1378.005450	17.488397
34.380099	1375.391934	17.493415
34.016623	1378.986733	17.498432
34.341867	1369.270132	17.503450
34.183539	1384.650681	17.508467
34.148937	1389.743261	17.513485
34.484062	1398.864283	17.518503
34.375820	1412.831283	17.523520
34.369646	1403.876606	17.528538
34.739075	1405.516323	17.533555
34.794429	1406.675344	17.538573
34.895536	1382.209824	17.543591
34.564530	1381.576673	17.548608
34.776808	1372.225143	17.553626
34.993671	1369.640915	17.558643
34.636862	1364.567240	17.563661
34.637525	1365.825046	17.568679
34.275919	1369.295733	17.573696
34.755283	1367.668368	17.578714
34.490788	1368.485815	17.583731
34.611414	1364.679886	17.588749
34.752172	1375.980125	17.593767
34.549950	1393.118455	17.598784
35.078566	1398.679692	17.603802
34.934141	1399.373771	17.608819
34.687711	1401.204418	17.613837
35.043217	1389.335491	17.618855
34.844147	1399.624547	17.623872
34.822571	1405.553830	17.628890
35.319057	1398.080224	17.633907
34.811668	1406.343777	17.638925
35.306706	1396.440858	17.643943
34.688377	1400.243302	17.648960
34.935217	1392.108895	17.653978
35.256491	1410.416844	17.658995
35.342351	1429.624416	17.664013
35.751642	1416.640053	17.669031
35.495968	1407.119411	17.674048
35.212670	1390.494773	17.679066
35.525139	1390.727777	17.684083
35.156542	1419.301940	17.689101
35.440761	1420.235966	17.694119
35.478079	1426.557629	17.699136
35.852098	1413.589922	17.704154
35.952697	1425.298152	17.709171
35.572490	1428.403084	17.714189
36.071451	1420.691693	17.719207
35.801647	1417.588560	17.724224
35.801589	1423.766028	17.729242
35.937801	1422.978317	17.734259
35.496441	1428.634116	17.739277
35.919878	1425.634304	17.744295
35.974762	1423.040620	17.749312
36.100516	1423.267281	17.754330
36.077954	1417.454006	17.759347
35.969346	1421.289332	17.764365
36.061188	1412.455439	17.769383
36.139873	1420.368646	17.774400
35.873724	1413.959698	17.779418
36.355455	1414.015935	17.784435
35.952389	1420.176941	17.789453
35.904420	1419.369870	17.794471
36.204672	1425.356395	17.799488
35.961130	1421.216005	17.804506
36.181080	1418.900511	17.809523
36.003431	1427.352069	17.814541
36.151751	1428.152670	17.819559
36.433914	1447.037317	17.824576
36.602932	1442.314256	17.829594
36.301666	1441.906862	17.834611
36.430057	1458.072854	17.839629
36.774801	1445.609097	17.844647
36.512410	1442.915894	17.849664
36.012503	1456.741388	17.854682
36.811907	1443.539999	17.859699
36.497016	1441.449281	17.864717
36.735756	1434.907095	17.869735
36.656714	1445.455243	17.874752
36.434013	1448.488291	17.879770
36.729841	1455.279967	17.884787
36.866764	1471.277264	17.889805
37.236395	1466.239589	17.894823
37.381947	1479.210126	17.899840
37.451572	1470.710138	17.904858
37.592877	1437.010110	17.909875
37.320259	1443.908904	17.914893
37.121274	1447.208859	17.919911
37.122148	1439.375270	17.924928
37.242090	1443.464720	17.929946
37.343655	1435.051389	17.934963
37.320634	1440.458363	17.939981
37.565965	1424.567469	17.944999
37.334508	1427.151241	17.950016
37.465020	1427.026578	17.955034
37.450572	1431.404924	17.960051
37.300658	1435.946188	17.965069
37.397253	1441.602648	17.970087
37.451920	1434.713771	17.975104
37.367513	1428.512149	17.980122
37.440727	1429.405268	17.985139
37.175096	1431.300107	17.990157
37.327857	1448.976796	17.995175
37.506159	1461.923799	18.000192
37.269660	1465.129382	18.005210
37.783654	1456.495939	18.010227
37.291703	1469.267333	18.015245
37.496372	1464.750940	18.020263
37.987573	1474.067836	18.025280
38.158526	1479.651992	18.030298
38.164169	1488.993042	18.035315
37.834439	1477.008380	18.040333
38.070980	1487.673870	18.045351
38.253830	1494.049846	18.050368
38.399534	1490.207267	18.055386
38.555549	1471.377774	18.060403
38.092573	1476.126076	18.065421
38.089071	1464.079051	18.070439
38.317508	1472.033670	18.075456
38.235867	1479.342194	18.080474
38.678432	1479.264965	18.085491
38.501265	1477.892516	18.090509
38.557408	1480.090631	18.095527
38.548964	1455.916482	18.100544
38.702506	1460.450120	18.105562
38.891891	1453.576761	18.110579
38.535185	1449.131884	18.115597
38.573204	1441.793066	18.120615
38.523049	1455.938274	18.125632
38.417456	1461.103821	18.130650
38.578229	1459.944978	18.135667
38.489136	1481.096204	18.140685
38.497794	1481.721885	18.145703
38.766952	1481.723698	18.150720
38.519577	1472.858437	18.155738
38.734477	1469.268366	18.160755
38.817868	1479.302168	18.165773
38.657981	1478.858617	18.170791
38.790027	1488.214207	18.175808
38.856750	1507.713580	18.180826
39.075151	1506.155502	18.185843
38.907827	1508.048866	18.190861
38.956918	1509.291793	18.195879
39.290553	1515.740879	18.200896
39.074936	1516.009388	18.205914
39.244058	1501.882922	18.210931
39.006515	1510.015927	18.215949
39.061325	1510.726095	18.220967
39.448833	1519.914703	18.225984
39.339212	1532.616671	18.231002
39.445195	1529.312460	18.236019
39.281894	1531.967651	18.241037
39.498196	1532.953650	18.246055
40.196221	1526.978153	18.251072
39.829803	1537.403010	18.256090
40.068398	1518.328350	18.261107
39.875379	1521.833802	18.266125
39.691026	1510.295102	18.271143
40.067304	1507.635500	18.276160
39.589108	1515.025121	18.281178
39.826660	1510.606809	18.286195
40.139378	1519.247818	18.291213
39.918692	1526.715739	18.296231
40.286947	1525.846377	18.301248
40.033313	1516.892768	18.306266
40.074656	1518.869744	18.311283
40.071954	1517.411580	18.316301
40.105914	1521.645949	18.321319
40.148811	1525.733784	18.326336
40.253621	1525.164809	18.331354
40.329361	1522.391309	18.336371
40.467914	1520.614569	18.341389
40.382078	1525.665471	18.346407
40.365093	1513.473610	18.351424
40.367917	1517.836727	18.356442
40.597748	1525.916913	18.361459
40.311808	1518.704220	18.366477
40.683290	1520.920890	18.371495
40.824229	1521.109221	18.376512
40.690612	1514.191195	18.381530
40.915794	1515.919516	18.386547
40.704090	1532.584046	18.391565
40.611018	1516.701740	18.396583
40.541578	1510.148254	18.401600
40.592036	1525.267898	18.406618
40.625043	1515.317255	18.411635
40.515751	1524.011077	18.416653
40.607116	1531.534309	18.421671
41.014823	1533.248018	18.426688
40.720335	1550.149050	18.431706
40.815256	1557.386708	18.436723
40.653856	1557.798403	18.441741
41.149426	1551.898275	18.446759
41.247146	1548.356286	18.451776
41.049990	1551.430009	18.456794
41.234811	1540.790577	18.461811
41.213188	1550.138138	18.466829
41.325612	1557.649046	18.471847
41.175853	1548.236780	18.476864
41.409226	1562.593464	18.481882
41.483732	1562.646929	18.486899
41.580981	1567.952589	18.491917
41.428477	1563.815421	18.496935
41.867739	1563.651349	18.501952
41.893056	1560.886371	18.506970
42.222700	1553.456795	18.511987
41.888130	1558.840896	18.517005
41.837624	1557.089095	18.522023
41.966862	1545.663485	18.527040
41.738899	1553.629402	18.532058
42.023947	1545.989119	18.537075
42.003120	1549.824143	18.542093
41.962643	1569.877651	18.547111
42.204052	1558.024891	18.552128
42.074838	1557.512105	18.557146
42.180846	1558.317737	18.562163
42.101879	1567.474420	18.567181
42.139937	1565.020087	18.572199
42.556380	1554.301628	18.577216
42.211301	1566.676640	18.582234
42.135721	1562.247272	18.587251
42.035695	1560.729607	18.592269
42.128956	1570.961219	18.597287
42.236416	1560.637861	18.602304
42.154668	1568.105674	18.607322
42.084390	1555.005589	18.612339
42.344317	1546.833903	18.617357
42.555808	1575.210345	18.622375
42.332593	1583.954321	18.627392
42.558119	1585.323588	18.632410
42.593568	1583.633751	18.637427
42.578660	1602.582442	18.642445
42.601317	1590.132036	18.647463
42.730732	1586.414548	18.652480
43.050853	1599.636026	18.657498
43.281163	1595.990040	18.662515
43.434513	1577.856627	18.667533
43.121785	1586.824816	18.672551
43.283136	1590.856878	18.677568
42.943598	1591.962879	18.682586
43.014743	1584.671071	18.687603
43.124894	1589.409331	18.692621
42.733138	1581.758449	18.697639
43.076628	1582.059549	18.702656
43.005558	1583.236130	18.707674
43.250824	1580.375362	18.712691
43.071665	1594.292837	18.717709
43.097500	1610.359417	18.722727
43.305351	1605.976888	18.727744
43.399856	1607.307383	18.732762
43.321361	1603.627005	18.737779
43.192285	1615.821499	18.742797
43.267988	1628.257127	18.747815
43.689252	1625.706984	18.752832
43.904881	1642.713165	18.757850
44.147978	1636.919481	18.762867
43.950380	1633.002710	18.767885
43.922046	1635.293339	18.772903
44.322081	1610.686731	18.777920
43.891359	1612.791328	18.782938
44.134988	1609.542099	18.787955
44.210242	1594.589836	18.792973
43.645868	1604.309167	18.797991
44.422630	1614.144238	18.803008
44.278444	1626.265658	18.808026
44.080196	1632.104357	18.813043
44.197929	1634.924120	18.818061
44.101050	1636.768856	18.823079
44.180154	1623.160235	18.828096
44.062744	1635.698833	18.833114
44.131626	1635.822903	18.838131
44.078882	1628.211632	18.843149
44.188442	1633.048219	18.848167
44.170818	1650.371261	18.853184
44.382167	1655.044203	18.858202
44.528839	1656.279480	18.863219
44.716314	1668.418164	18.868237
44.896528	1662.213462	18.873255
45.097988	1654.758963	18.878272
44.683895	1663.402851	18.883290
44.715662	1648.313451	18.888307
45.376321	1649.385061	18.893325
44.818964	1660.589091	18.898343
44.780719	1654.612396	18.903360
44.847235	1654.335139	18.908378
45.035130	1655.629736	18.913395
45.059289	1655.258706	18.918413
44.875408	1660.380177	18.923431
45.367753	1676.928519	18.928448
45.460985	1679.232527	18.933466
45.545832	1676.380339	18.938483
45.848238	1667.808512	18.943501
45.606517	1649.882210	18.948519
45.769761	1639.407868	18.953536
45.246412	1655.219427	18.958554
45.270827	1647.921140	18.963571
45.657769	1643.475152	18.968589
45.411198	1655.226952	18.973607
45.458392	1656.315697	18.978624
45.733062	1666.641787	18.983642
45.507844	1680.168580	18.988659
45.750302	1678.856083	18.993677
45.925339	1674.595280	18.998695
46.141217	1680.542509	19.003712
46.052563	1678.696027	19.008730
45.882186	1683.769415	19.013747
46.028944	1673.553842	19.018765
45.947218	1683.856172	19.023783
46.054783	1680.873279	19.028800
45.945504	1685.236860	19.033818
45.948608	1681.838805	19.038835
46.405584	1673.195769	19.043853
46.221334	1678.236019	19.048871
46.183997	1668.331740	19.053888
45.979499	1679.171412	19.058906
46.143548	1700.810368	19.063923
46.343571	1698.245994	19.068941
46.133604	1714.659285	19.073959
46.563716	1706.051375	19.078976
46.478458	1701.291327	19.083994
46.611509	1706.901117	19.089011
47.129145	1702.042032	19.094029
46.784003	1703.175734	19.099047
46.630439	1703.824885	19.104064
46.577730	1709.555519	19.109082
46.932832	1711.890658	19.114099
47.388557	1715.354688	19.119117
47.161551	1727.121024	19.124135
46.986831	1720.591930	19.129152
47.000679	1717.502091	19.134170
47.087888	1718.886747	19.139187
47.743242	1734.391418	19.144205
47.416471	1729.696071	19.149223
47.391032	1702.879804	19.154240
47.319500	1702.520648	19.159258
47.337295	1720.883449	19.164275
47.702526	1716.964779	19.169293
47.354485	1722.966633	19.174311
47.560451	1731.493924	19.179328
47.630104	1723.914735	19.184346
47.631311	1727.696364	19.189363
47.784460	1724.706520	19.194381
47.587087	1723.151979	19.199399
47.475074	1729.583866	19.204416
47.820859	1724.508124	19.209434
47.584300	1726.347413	19.214451
47.956906	1722.897343	19.219469
47.823747	1728.196061	19.224487
47.409651	1722.957738	19.229504
47.595851	1722.520761	19.234522
47.635252	1741.159113	19.239539
48.218606	1748.215767	19.244557
48.065255	1742.798343	19.249575
47.842267	1753.262234	19.254592
48.247835	1750.747536	19.259610
47.747737	1752.053089	19.264627
48.317825	1752.893249	19.269645
48.069723	1757.547670	19.274663
48.618743	1767.824950	19.279680
48.569149	1770.110059	19.284698
48.254393	1772.885386	19.289715
48.780316	1775.575132	19.294733
48.857663	1773.722464	19.299751
49.001318	1775.707760	19.304768
49.398230	1771.798603	19.309786
48.681595	1756.532020	19.314803
48.898639	1736.156292	19.319821
49.074898	1743.925211	19.324839
48.761316	1730.407958	19.329856
48.652665	1744.025175	19.334874
48.744548	1757.787196	19.339891
49.275769	1762.020158	19.344909
49.024985	1767.865424	19.349927
49.072380	1765.780927	19.354944
49.256287	1761.323384	19.359962
49.315019	1762.476757	19.364979
49.640348	1744.221040	19.369997
49.466173	1756.160140	19.375015
49.445247	1760.941961	19.380032
49.459034	1760.656883	19.385050
49.162199	1772.959135	19.390067
49.447816	1756.340665	19.395085
49.530522	1765.986825	19.400103
49.398272	1763.684210	19.405120
49.456357	1773.473402	19.410138
49.438849	1783.920876	19.415155
49.777043	1783.654818	19.420173
49.703284	1797.833371	19.425191
49.595298	1792.737526	19.430208
50.013058	1781.486279	19.435226
49.516201	1802.753158	19.440243
50.016519	1792.728656	19.445261
49.902122	1794.635943	19.450279
50.216138	1821.116409	19.455296
50.432161	1813.295890	19.460314
50.110525	1815.485032	19.465331
50.664830	1819.198511	19.470349
50.908408	1819.869431	19.475367
50.528084	1815.602933	19.480384
50.672606	1796.342122	19.485402
50.614092	1787.899350	19.490419
50.739263	1778.021091	19.495437
50.472232	1780.089999	19.500455
50.225653	1784.506412	19.505472
50.388583	1800.032884	19.510490
50.678478	1815.214022	19.515507
50.812566	1813.355516	19.520525
50.884900	1816.866982	19.525543
50.910288	1819.577842	19.530560
51.140015	1814.599193	19.535578
50.681841	1818.399678	19.540595
50.839785	1821.385053	19.545613
50.889846	1818.451985	19.550631
50.866440	1819.813990	19.555648
51.359921	1829.723764	19.560666
51.078513	1838.105696	19.565683
51.497284	1835.375245	19.570701
51.483256	1841.507754	19.575719
51.342208	1837.860291	19.580736
51.887020	1831.402579	19.585754
51.944234	1836.451989	19.590771
51.952850	1835.865832	19.595789
51.753261	1822.511134	19.600807
51.702325	1809.604265	19.605824
51.700542	1807.391488	19.610842
51.877808	1828.152762	19.615859
52.081446	1829.051711	19.620877
51.576357	1817.806302	19.625895
51.299293	1829.972475	19.630912
51.698247	1827.283682	19.635930
51.829511	1841.986988	19.640947
51.630774	1834.678249	19.645965
51.873541	1833.708560	19.650983
51.804612	1840.407159	19.656000
52.246038	1848.012052	19.661018
52.355611	1863.841268	19.666035
52.395695	1857.843873	19.671053
52.395201	1855.431097	19.676071
52.167473	1863.178854	19.681088
52.531657	1853.048282	19.686106
52.347401	1860.798105	19.691123
52.078207	1872.202473	19.696141
52.018286	1857.118374	19.701159
52.529600	1863.778966	19.706176
53.133265	1880.597484	19.711194
53.231229	1879.249014	19.716211
53.199401	1860.356003	19.721229
53.346723	1853.920665	19.726247
52.995771	1849.801647	19.731264
53.118336	1839.726757	19.736282
52.994949	1856.528795	19.741299
52.886085	1854.675004	19.746317
53.258166	1843.267107	19.751335
53.122113	1851.666753	19.756352
53.543463	1866.089498	19.761370
53.089804	1864.154903	19.766387
53.468569	1870.531336	19.771405
53.493203	1883.955412	19.776423
53.202366	1879.025368	19.781440
53.562881	1875.731378	19.786458
53.458031	1881.033343	19.791475
53.358530	1880.464461	19.796493
53.641261	1873.333394	19.801511
53.432268	1886.664008	19.806528
53.714730	1884.725864	19.811546
53.719986	1885.084833	19.816563
53.828861	1895.754383	19.821581
53.792826	1911.465403	19.826599
53.879781	1910.847796	19.831616
54.157069	1903.034232	19.836634
53.945963	1912.547758	19.841651
54.204084	1910.010358	19.846669
54.253406	1907.559030	19.851687
54.078579	1910.112856	19.856704
54.109261	1909.428180	19.861722
54.128512	1914.420707	19.866739
54.216137	1913.586874	19.871757
54.363672	1915.921309	19.876775
53.988525	1923.895598	19.881792
54.487736	1939.651647	19.886810
54.558666	1933.969365	19.891827
54.597233	1930.269366	19.896845
54.941786	1928.517390	19.901863
54.571317	1930.519366	19.906880
54.622859	1927.575993	19.911898
54.906890	1946.231052	19.916915
55.113046	1951.296040	19.921933
55.549832	1955.098650	19.926951
55.350763	1955.142999	19.931968
55.092904	1928.472411	19.936986
55.100741	1933.054871	19.942003
55.271459	1947.793683	19.947021
55.340681	1954.906262	19.952039
55.303556	1950.738508	19.957056
55.436202	1945.488097	19.962074
55.611826	1952.315604	19.967091
55.317759	1948.445988	19.972109
55.890872	1947.454574	19.977127
55.559079	1949.546999	19.982144
55.968260	1941.746065	19.987162
55.627553	1943.787213	19.992179
55.200500	1947.466458	19.997197
55.499145	1943.023363	20.002215
55.407283	1954.800410	20.007232
55.585172	1951.178553	20.012250
55.579812	1966.347811	20.017267
55.587286	1982.167448	20.022285
56.119428	1973.394516	20.027303
56.122884	1979.990279	20.032320
55.970103	1972.901807	20.037338
56.083297	1973.201804	20.042355
56.274589	1974.792487	20.047373
56.433530	1990.788656	20.052391
56.556482	2001.983846	20.057408
56.791750	1994.682240	20.062426
56.702860	1999.564136	20.067443
56.929332	2009.099496	20.072461
57.234850	1991.853538	20.077479
56.931102	1976.172679	20.082496
56.941907	1947.549808	20.087514
56.822085	1953.682326	20.092531
56.312060	1982.270076	20.097549
56.930670	1981.569730	20.102567
56.820408	1991.240439	20.107584
57.155840	1987.046736	20.112602
57.208973	2000.037316	20.117619
57.219218	2004.640656	20.122637
57.368763	1989.578895	20.127655
57.445783	2007.047114	20.132672
57.452718	1999.440165	20.137690
57.290041	1989.958314	20.142707
57.227485	1995.452520	20.147725
57.762346	1998.836814	20.152743
57.407335	2005.956929	20.157760
57.562832	2001.654192	20.162778
57.755898	2004.866845	20.167795
57.786376	2021.717841	20.172813
57.803939	2024.962649	20.177831
57.924398	2021.275471	20.182848
58.002525	2017.608280	20.187866
58.145680	2013.186727	20.192883
57.646009	2020.179983	20.197901
57.923613	2021.147224	20.202919
58.021323	2021.941065	20.207936
57.763785	2023.646862	20.212954
57.941699	2028.124875	20.217971
58.095297	2039.938385	20.222989
58.281763	2047.727620	20.228007
58.157020	2045.525090	20.233024
58.143333	2041.570539	20.238042
58.279876	2054.184822	20.243059
58.084354	2051.243084	20.248077
58.691962	2055.897514	20.253095
58.589922	2069.856802	20.258112
58.738122	2069.115892	20.263130
59.140538	2078.275605	20.268147
59.090061	2084.446907	20.273165
59.339141	2068.025458	20.278183
59.255758	2080.831600	20.283200
59.140080	2070.792779	20.288218
59.375426	2065.612749	20.293235
59.160348	2072.840860	20.298253
58.739752	2066.563840	20.303271
59.028893	2066.002768	20.308288
59.238952	2055.113759	20.313306
59.605494	2064.239632	20.318323
59.405497	2064.567176	20.323341
59.463393	2060.772033	20.328359
59.209992	2083.160554	20.333376
59.763500	2093.551080	20.338394
59.878072	2098.625346	20.343411
59.770555	2109.397133	20.348429
59.957164	2113.463542	20.353447
59.856064	2103.987388	20.358464
59.939583	2103.635275	20.363482
59.869335	2098.931081	20.368499
59.680030	2105.866593	20.373517
60.041524	2097.123758	20.378535
59.895147	2102.018335	20.383552
60.291243	2104.807539	20.388570
60.234259	2091.171786	20.393587
60.084864	2113.876791	20.398605
60.212976	2117.576332	20.403623
60.474762	2125.449213	20.408640
60.425206	2127.194661	20.413658
60.515510	2129.801551	20.418675
60.461151	2133.719024	20.423693
60.994308	2116.414447	20.428711
60.783737	2114.736862	20.433728
60.735074	2118.637841	20.438746
60.557517	2125.636571	20.443763
60.744648	2147.256004	20.448781
60.601773	2152.745233	20.453799
60.737432	2152.187869	20.458816
61.084844	2153.299866	20.463834
61.109263	2154.929757	20.468851
60.872860	2159.694558	20.473869
61.580947	2167.318138	20.478887
61.692856	2182.011189	20.483904
61.693299	2186.473895	20.488922
62.108954	2171.119583	20.493939
61.835975	2151.070321	20.498957
61.962289	2146.809763	20.503975
62.067536	2144.482608	20.508992
61.962013	2143.618088	20.514010
62.005778	2147.358539	20.519027
62.031302	2145.719488	20.524045
62.059514	2133.626349	20.529063
62.146253	2134.140345	20.534080
61.826686	2144.007728	20.539098
62.196625	2140.818414	20.544115
62.212355	2161.516486	20.549133
62.106762	2166.340374	20.554151
62.177966	2160.725869	20.559168
62.183730	2169.087884	20.564186
62.410380	2167.040240	20.569203
62.633347	2173.285277	20.574221
62.688344	2171.810234	20.579239
62.234747	2180.111562	20.584256
62.113818	2175.475360	20.589274
62.750817	2181.237261	20.594291
62.660344	2204.623342	20.599309
62.637876	2208.707791	20.604327
62.815263	2197.564855	20.609344
62.734716	2196.340531	20.614362
62.853612	2205.872336	20.619379
62.494981	2204.584722	20.624397
63.133993	2208.894871	20.629415
63.337936	2214.616742	20.634432
63.155820	2226.762616	20.639450
63.639032	2222.780234	20.644467
63.577061	2220.525183	20.649485
64.042792	2214.160099	20.654503
63.905539	2213.998387	20.659520
63.531577	2231.629367	20.664538
63.970382	2208.640047	20.669555
64.194120	2213.879954	20.674573
63.940536	2215.161538	20.679591
64.063032	2201.694238	20.684608
63.616376	2205.215380	20.689626
64.169722	2209.015327	20.694643
63.968934	2220.421835	20.699661
64.201232	2206.470486	20.704679
64.053403	2201.756643	20.709696
64.275541	2214.524613	20.714714
64.448766	2210.008477	20.719731
63.821797	2212.385320	20.724749
63.937565	2205.284053	20.729767
64.159689	2230.353975	20.734784
64.270278	2240.350712	20.739802
64.632953	2240.998428	20.744819
64.443858	2258.294785	20.749837
64.396040	2243.687594	20.754855
64.841859	2242.612483	20.759872
64.492725	2259.148553	20.764890
64.589875	2262.233619	20.769907
64.774387	2270.283304	20.774925
64.835477	2272.498233	20.779943
65.088655	2280.025995	20.784960
65.005811	2277.177591	20.789978
65.174477	2273.987065	20.794995
64.814908	2299.952753	20.800013
65.295695	2296.939363	20.805031
65.789111	2294.572252	20.810048
65.455649	2307.138831	20.815066
65.515121	2298.884136	20.820083
65.490080	2300.169689	20.825101
65.924165	2307.625842	20.830119
65.797928	2303.850241	20.835136
65.680747	2301.665713	20.840154
65.944323	2305.564351	20.845171
65.898706	2318.565612	20.850189
66.501790	2313.369610	20.855207
66.508038	2303.134522	20.860224
66.403954	2325.129265	20.865242
66.499094	2317.064318	20.870259
66.388784	2307.499412	20.875277
66.638695	2320.620132	20.880295
66.458889	2314.107963	20.885312
66.300163	2320.797004	20.890330
66.726390	2313.845745	20.895347
66.704699	2317.710824	20.900365
66.494682	2313.906942	20.905383
66.920587	2308.878790	20.910400
66.782064	2324.993352	20.915418
66.842418	2310.458568	20.920435
66.945527	2319.030936	20.925453
66.795859	2317.738504	20.930471
66.980061	2323.072179	20.935488
66.905945	2332.836725	20.940506
67.142896	2335.447762	20.945523
67.152078	2340.546608	20.950541
66.912816	2339.740984	20.955559
67.268984	2341.324538	20.960576
67.458825	2355.820052	20.965594
67.427224	2360.503044	20.970611
67.791589	2363.864616	20.975629
67.755934	2370.064879	20.980647
67.856998	2361.161012	20.985664
67.643739	2367.212292	20.990682
67.613732	2355.125254	20.995699
67.629240	2368.982127	21.000717
68.056876	2369.789375	21.005735
68.250607	2358.933557	21.010752
68.081507	2361.877420	21.015770
68.199810	2360.988695	21.020787
67.994960	2374.715860	21.025805
68.275828	2384.160779	21.030823
68.028293	2389.348910	21.035840
68.435840	2396.989200	21.040858
68.585899	2384.512376	21.045875
69.045890	2389.097413	21.050893
68.972969	2385.246452	21.055911
69.175048	2376.257583	21.060928
69.397876	2372.199894	21.065946
69.467501	2378.552631	21.070963
69.197351	2376.689406	21.075981
69.204456	2377.278770	21.080999
69.549161	2369.599093	21.086016
69.269713	2382.780964	21.091034
69.390709	2367.923338	21.096051
69.387286	2392.918600	21.101069
69.307953	2372.304617	21.106087
69.377281	2363.634122	21.111104
69.092793	2375.040993	21.116122
69.404138	2375.477729	21.121139
69.665426	2380.937847	21.126157
69.733325	2391.660570	21.131175
70.281288	2398.223223	21.136192
69.795156	2403.470666	21.141210
69.831813	2397.725772	21.146227
69.886034	2393.442417	21.151245
69.673024	2404.216883	21.156263
70.114643	2405.857971	21.161280
70.005076	2403.936321	21.166298
70.429006	2420.417842	21.171315
70.209702	2429.561221	21.176333
70.381731	2435.160113	21.181351
70.568774	2427.422807	21.186368
70.426488	2436.632393	21.191386
70.413436	2431.235043	21.196403
70.436225	2429.116139	21.201421
70.341807	2429.123709	21.206439
70.611838	2449.731921	21.211456
70.544332	2464.154521	21.216474
70.806503	2455.359203	21.221491
71.013478	2457.458917	21.226509
70.890220	2454.745494	21.231527
71.197728	2462.437386	21.236544
71.205731	2477.298270	21.241562
71.540164	2471.629919	21.246579
71.692378	2478.861497	21.251597
71.596676	2480.175669	21.256615
72.007494	2474.898402	21.261632
71.628413	2479.523506	21.266650
71.682799	2477.382643	21.271667
72.078370	2476.544740	21.276685
71.757651	2492.754736	21.281703
72.154692	2479.798474	21.286720
71.859278	2480.796660	21.291738
72.120106	2475.795143	21.296755
72.282826	2475.722036	21.301773
71.921236	2480.482821	21.306791
72.131488	2486.871020	21.311808
72.369998	2495.426820	21.316826
72.394552	2499.885041	21.321843
72.702001	2505.595823	21.326861
72.470401	2502.581226	21.331879
72.549341	2506.465153	21.336896
72.566017	2508.983101	21.341914
72.584874	2497.189625	21.346931
72.987924	2493.157237	21.351949
72.658193	2503.718795	21.356967
73.072166	2504.352338	21.361984
72.741524	2504.807769	21.367002
72.877040	2526.973623	21.372019
73.234291	2536.186739	21.377037
73.289843	2532.918205	21.382055
73.329591	2531.583432	21.387072
73.427593	2533.545075	21.392090
73.127264	2534.488372	21.397107
73.677092	2529.629027	21.402125
73.724008	2533.863895	21.407143
73.791711	2541.854291	21.412160
73.861242	2558.241778	21.417178
73.956973	2563.643696	21.422195
74.174957	2557.842206	21.427213
74.115646	2557.133793	21.432231
74.495374	2552.713542	21.437248
74.497190	2556.372055	21.442266
74.200051	2556.147986	21.447283
74.660337	2546.751812	21.452301
74.204220	2550.848173	21.457319
74.029029	2560.620511	21.462336
74.207507	2562.356670	21.467354
74.396751	2554.799632	21.472371
74.654232	2580.076862	21.477389
74.535001	2585.933175	21.482407
74.945802	2577.500994	21.487424
74.988276	2586.553377	21.492442
75.080043	2588.072585	21.497459
75.206634	2573.037473	21.502477
75.054051	2578.702458	21.507495
75.308214	2578.860876	21.512512
75.166624	2586.850449	21.517530
75.235128	2586.769094	21.522547
75.094875	2596.722478	21.527565
75.077834	2615.393653	21.532583
75.498095	2607.944073	21.537600
75.449058	2616.073277	21.542618
75.710350	2611.811940	21.547635
75.797620	2601.323126	21.552653
75.405950	2617.511710	21.557671
75.727759	2626.040039	21.562688
76.117031	2627.102837	21.567706
75.999374	2643.333958	21.572723
76.374178	2636.010962	21.577741
76.078446	2632.375091	21.582759
76.473138	2630.173054	21.587776
76.570274	2627.546204	21.592794
76.483188	2636.697775	21.597811
76.476028	2644.704728	21.602829
76.797070	2652.642689	21.607847
76.744150	2657.085217	21.612864
76.945131	2672.902521	21.617882
76.978466	2670.120470	21.622899
77.288754	2653.677263	21.627917
76.912794	2659.138459	21.632935
77.021239	2657.722446	21.637952
77.283426	2657.212853	21.642970
76.932436	2661.688496	21.647987
77.087767	2654.155319	21.653005
77.484335	2666.660015	21.658023
77.566504	2680.172120	21.663040
77.491178	2683.309392	21.668058
77.466566	2686.812275	21.673075
77.521956	2682.993183	21.678093
77.313949	2692.712763	21.683111
77.964424	2679.581789	21.688128
77.857500	2684.653875	21.693146
78.160440	2682.855548	21.698163
78.422067	2676.497431	21.703181
78.616400	2674.955618	21.708199
78.179513	2679.887162	21.713216
78.101119	2680.015697	21.718234
78.178771	2687.131946	21.723251
78.591733	2686.286828	21.728269
78.430479	2701.575673	21.733287
78.435350	2700.445454	21.738304
78.570977	2696.767420	21.743322
78.153219	2695.366904	21.748339
78.953714	2704.741312	21.753357
78.604062	2725.049955	21.758375
79.090637	2731.351654	21.763392
78.819508	2720.739120	21.768410
79.126140	2730.577803	21.773427
79.197268	2723.493321	21.778445
79.214457	2733.051313	21.783463
79.137366	2737.106741	21.788480
79.966565	2744.789334	21.793498
79.473694	2760.045048	21.798515
79.639521	2758.148117	21.803533
79.680453	2758.052420	21.808551
79.929083	2769.953930	21.813568
80.081617	2767.301762	21.818586
79.976445	2762.537589	21.823603
80.043838	2753.296366	21.828621
80.056091	2754.859634	21.833639
80.001137	2761.265986	21.838656
80.372026	2778.711124	21.843674
80.448147	2793.732699	21.848691
80.636170	2793.618995	21.853709
80.437398	2788.542349	21.858727
80.643327	2780.920243	21.863744
80.636703	2786.519455	21.868762
80.456518	2790.128970	21.873779
80.732853	2783.505402	21.878797
80.954349	2804.140021	21.883815
80.826445	2815.793174	21.888832
81.367741	2807.150341	21.893850
81.012434	2818.154107	21.898867
81.172301	2817.631694	21.903885
81.606486	2821.649507	21.908903
81.484550	2814.369341	21.913920
81.665988	2801.105152	21.918938
81.697392	2808.427119	21.923955
81.555975	2805.777851	21.928973
81.494803	2806.449769	21.933991
81.343023	2829.871923	21.939008
81.840538	2830.138942	21.944026
82.001504	2838.799276	21.949043
82.196708	2838.815481	21.954061
81.821260	2847.312898	21.959079
81.684707	2847.822481	21.964096
82.214836	2863.440717	21.969114
82.355175	2858.849319	21.974131
82.511000	2869.558436	21.979149
82.687958	2867.868302	21.984167
82.543120	2863.701171	21.989184
82.856276	2864.303362	21.994202
83.062136	2862.372640	21.999219
83.030043	2860.619813	22.004237
82.594486	2868.624054	22.009255
83.002992	2880.608279	22.014272
83.621795	2887.102551	22.019290
83.333104	2897.344618	22.024307
83.582730	2897.537253	22.029325
83.315480	2891.405804	22.034343
83.305979	2903.915395	22.039360
83.523925	2902.337770	22.044378
82.991556	2899.258233	22.049395
83.469432	2889.408971	22.054413
83.468869	2894.598189	22.059431
83.360367	2918.805409	22.064448
83.260108	2921.908859	22.069466
83.681140	2922.733765	22.074483
83.855191	2927.525262	22.079501
83.903728	2956.586259	22.084519
83.946455	2968.607768	22.089536
84.606816	2944.204636	22.094554
84.615319	2949.376627	22.099571
84.884179	2953.132044	22.104589
84.613790	2947.126676	22.109607
84.606903	2946.901880	22.114624
84.937072	2958.743213	22.119642
84.903870	2971.590617	22.124659
85.471791	2967.291900	22.129677
85.337297	2967.709025	22.134695
85.230592	2977.067572	22.139712
85.589195	2965.449083	22.144730
85.578645	2970.776190	22.149747
85.572802	2973.278251	22.154765
85.593020	2963.571887	22.159783
85.587132	2967.097919	22.164800
85.785621	2970.598053	22.169818
85.709965	2969.921257	22.174835
85.745312	2970.313860	22.179853
85.787447	2970.152612	22.184871
85.962258	2966.776292	22.189888
86.234317	2964.091348	22.194906
85.592822	2980.378479	22.199923
85.590257	2992.270490	22.204941
86.065827	2996.134274	22.209959
86.117607	3011.669507	22.214976
86.213570	3010.828530	22.219994
86.489697	3028.462041	22.225011
86.635842	3031.989736	22.230029
86.400559	3026.069083	22.235047
86.250303	3036.487570	22.240064
86.689959	3047.551859	22.245082
86.899166	3055.710665	22.250099
86.856397	3060.241587	22.255117
86.855992	3062.001458	22.260135
86.913350	3067.170533	22.265152
87.530239	3079.777538	22.270170
87.320962	3100.017611	22.275187
87.364240	3092.700958	22.280205
87.841048	3084.010363	22.285223
87.404843	3085.638714	22.290240
87.675474	3080.016710	22.295258
87.914694	3110.184232	22.300275
88.149634	3124.980286	22.305293
88.216509	3116.847550	22.310311
88.669302	3117.107794	22.315328
88.726822	3103.686272	22.320346
88.611136	3115.962016	22.325363
88.856982	3112.800295	22.330381
89.111185	3114.207089	22.335399
89.148437	3090.975546	22.340416
89.362854	3068.752906	22.345434
88.736461	3076.018348	22.350451
88.448508	3071.250821	22.355469
88.508252	3079.344970	22.360487
88.610767	3104.473083	22.365504
88.760556	3095.621174	22.370522
88.665989	3110.037822	22.375539
88.988794	3110.075854	22.380557
89.201831	3125.039301	22.385575
88.905825	3131.675394	22.390592
89.494926	3136.783397	22.395610
89.504906	3134.135432	22.400627
89.311203	3133.007287	22.405645
89.335979	3147.503852	22.410663
89.758597	3160.465060	22.415680
90.157657	3161.264872	22.420698
90.013584	3174.912232	22.425715
89.924442	3165.634427	22.430733
90.086085	3180.939086	22.435751
90.020806	3197.719001	22.440768
90.304271	3198.024155	22.445786
90.151337	3202.763080	22.450803
90.120415	3196.681038	22.455821
90.502965	3208.936728	22.460839
90.597510	3220.458154	22.465856
90.914688	3222.168321	22.470874
91.526319	3217.400912	22.475891
91.365121	3222.216797	22.480909
91.542766	3220.776504	22.485927
91.465239	3208.254343	22.490944
91.695951	3206.333645	22.495962
91.774898	3215.805748	22.500979
91.707767	3216.886135	22.505997
91.786375	3201.187105	22.511015
91.721175	3210.509408	22.516032
92.124574	3202.028509	22.521050
92.326303	3205.258093	22.526067
91.978161	3205.690055	22.531085
92.035012	3211.310427	22.536103
92.102908	3222.690595	22.541120
92.177650	3226.568311	22.546138
92.447815	3229.801552	22.551155
92.464213	3227.797371	22.556173
92.559867	3230.781111	22.561191
92.801233	3238.723289	22.566208
92.559898	3244.672859	22.571226
92.466249	3246.208008	22.576243
93.081636	3260.324811	22.581261
92.837060	3266.078474	22.586279
92.854752	3273.760002	22.591296
93.118286	3268.694597	22.596314
93.070257	3276.566508	22.601331
93.028515	3297.405514	22.606349
93.394613	3295.035674	22.611367
93.314887	3299.724344	22.616384
93.641266	3301.699133	22.621402
93.733753	3299.272146	22.626419
93.930199	3303.649441	22.631437
94.173217	3315.791268	22.636455
94.130970	3335.322177	22.641472
94.179637	3333.562644	22.646490
94.119181	3335.376562	22.651507
94.249441	3334.584229	22.656525
94.119583	3322.861154	22.661543
94.244855	3332.498503	22.666560
94.690870	3325.823441	22.671578
94.805482	3355.442362	22.676595
94.479647	3359.717397	22.681613
94.954084	3348.108222	22.686631
95.094080	3348.997703	22.691648
94.942275	3358.880061	22.696666
95.137845	3357.406873	22.701683
95.160976	3346.638790	22.706701
95.091059	3344.439808	22.711719
95.382885	3365.272209	22.716736
95.665931	3376.274427	22.721754
95.926548	3389.355902	22.726771
95.664949	3383.405209	22.731789
95.986236	3369.172567	22.736807
95.948500	3378.677830	22.741824
95.975570	3375.979756	22.746842
96.236802	3376.325202	22.751859
95.917197	3371.953353	22.756877
96.116696	3380.003307	22.761895
95.979231	3408.678966	22.766912
96.214748	3402.199675	22.771930
96.526190	3404.321825	22.776947
96.245470	3400.219520	22.781965
96.447222	3419.694468	22.786983
96.960175	3429.980795	22.792000
96.976461	3423.839682	22.797018
97.413065	3426.010837	22.802035
97.308843	3430.481158	22.807053
97.727448	3423.709797	22.812071
97.454607	3424.737183	22.817088
97.869538	3421.618720	22.822106
97.944552	3415.995848	22.827123
98.126991	3423.575820	22.832141
97.855236	3410.353321	22.837159
98.318559	3414.799933	22.842176
97.834642	3416.886978	22.847194
97.989043	3412.387581	22.852211
97.905424	3424.246073	22.857229
98.185912	3419.350650	22.862247
98.345072	3437.473237	22.867264
98.365116	3438.401835	22.872282
98.426578	3434.806354	22.877299
98.366838	3445.423539	22.882317
98.371670	3456.797765	22.887335
98.557225	3477.842756	22.892352
98.470452	3477.251631	22.897370
98.826971	3487.657939	22.902387
98.838516	3488.860380	22.907405
98.862169	3493.893044	22.912423
99.113287	3509.250564	22.917440
99.068389	3508.386774	22.922458
99.535937	3520.476307	22.927475
99.210974	3537.614850	22.932493
99.654839	3541.716293	22.937511
99.800248	3539.356113	22.942528
99.394361	3543.499939	22.947546
99.490521	3561.357888	22.952563
99.968474	3563.746244	22.957581
100.140856	3566.624458	22.962599
100.245753	3574.115742	22.967616
99.941429	3577.211310	22.972634
100.704517	3580.883247	22.977651
100.396539	3599.882813	22.982669
100.660685	3592.472736	22.987687
100.763536	3594.450642	22.992704
100.732886	3595.929353	22.997722
100.913615	3593.660571	23.002739
101.150037	3625.065767	23.007757
101.273717	3624.041833	23.012775
101.253308	3615.588222	23.017792
101.405387	3627.374064	23.022810
101.991432	3612.611235	23.027827
101.713496	3617.997707	23.032845
101.578823	3611.805875	23.037863
101.783497	3620.799580	23.042880
101.819602	3610.636253	23.047898
102.114843	3615.464631	23.052915
101.824943	3636.903361	23.057933
102.005204	3640.131466	23.062951
102.274445	3650.691281	23.067968
102.405472	3651.140531	23.072986
102.468966	3647.817498	23.078003
102.366390	3656.330895	23.083021
102.483081	3665.419085	23.088039
102.608709	3672.134160	23.093056
102.547743	3672.321830	23.098074
102.649588	3674.707785	23.103091
102.695962	3692.539466	23.108109
102.687717	3699.318800	23.113127
102.903536	3697.331607	23.118144
103.100172	3705.585353	23.123162
103.458045	3725.442760	23.128179
103.612489	3733.967272	23.133197
103.611092	3725.743531	23.138215
103.699722	3723.104910	23.143232
103.798085	3730.927665	23.148250
104.243958	3738.706386	23.153267
104.167639	3757.688731	23.158285
104.433358	3753.167691	23.163303
104.727556	3756.552191	23.168320
104.190092	3757.738678	23.173338
104.974437	3745.984692	23.178355
104.991829	3758.750765	23.183373
104.903065	3752.235542	23.188391
105.016358	3758.657024	23.193408
104.546165	3754.440657	23.198426
105.178264	3759.259087	23.203443
105.254788	3774.644933	23.208461
105.480879	3782.148182	23.213479
105.429030	3775.222124	23.218496
105.491580	3777.640572	23.223514
105.817568	3778.489502	23.228531
105.418923	3789.347963	23.233549
105.771562	3801.348042	23.238567
106.316503	3805.331279	23.243584
105.702090	3812.537992	23.248602
106.416049	3802.618831	23.253619
106.092885	3806.483702	23.258637
105.933600	3812.208511	23.263655
106.318935	3824.130764	23.268672
106.308456	3843.866118	23.273690
106.795556	3843.114010	23.278707
106.848405	3851.936085	23.283725
106.758115	3847.731327	23.288743
106.869632	3863.546915	23.293760
106.831132	3872.929376	23.298778
107.050484	3865.758463	23.303795
107.253759	3875.765548	23.308813
107.504175	3873.060011	23.313831
108.085998	3891.210927	23.318848
107.973241	3903.976183	23.323866
108.160060	3892.969648	23.328883
108.183041	3895.513158	23.333901
108.258496	3898.162566	23.338919
108.240423	3887.444619	23.343936
108.187657	3894.509744	23.348954
108.556788	3884.564046	23.353971
108.511690	3887.829440	23.358989
108.478806	3892.211726	23.364007
108.440908	3884.887641	23.369024
108.210550	3890.443513	23.374042
108.773773	3905.987258	23.379059
109.058160	3918.823518	23.384077
108.677179	3922.372376	23.389095
108.970364	3919.643622	23.394112
109.035792	3936.848018	23.399130
109.280492	3927.013013	23.404147
109.045581	3937.551998	23.409165
109.372366	3948.211564	23.414183
109.814469	3945.451112	23.419200
109.793660	3945.738057	23.424218
109.962284	3943.955090	23.429235
110.124957	3956.294557	23.434253
110.436593	3968.373983	23.439271
110.433355	3966.128854	23.444288
110.342653	3984.564631	23.449306
110.940302	3975.560265	23.454323
110.667313	3976.141640	23.459341
110.868392	3974.644650	23.464359
110.999646	3967.102415	23.469376
110.658944	3976.145499	23.474394
110.991976	3972.401081	23.479411
110.952488	3975.302176	23.484429
110.890422	3982.257065	23.489447
111.298346	3991.720952	23.494464
111.176937	3994.775747	23.499482
111.478902	3988.324603	23.504499
111.241888	4019.116690	23.509517
111.166721	4030.925034	23.514535
111.644186	4025.009060	23.519552
111.671875	4028.237654	23.524570
111.916015	4047.497327	23.529587
111.872091	4050.736970	23.534605
112.197217	4059.452754	23.539623
112.379129	4057.004967	23.544640
112.392692	4080.520584	23.549658
112.427037	4085.152058	23.554675
112.397437	4085.834561	23.559693
112.776967	4080.088689	23.564711
113.489421	4090.844472	23.569728
113.201092	4113.385591	23.574746
113.240900	4102.720531	23.579763
113.561730	4109.491732	23.584781
113.693845	4104.637542	23.589799
114.195215	4101.124339	23.594816
113.657210	4108.508330	23.599834
114.049739	4112.748728	23.604851
114.145136	4111.195170	23.609869
113.884967	4104.310475	23.614887
114.140163	4115.119391	23.619904
113.952846	4130.438552	23.624922
114.000365	4125.481009	23.629939
114.521485	4138.314555	23.634957
114.205897	4143.120012	23.639975
114.648813	4159.250835	23.644992
114.474788	4162.088366	23.650010
114.836355	4156.283229	23.655027
114.958565	4173.138337	23.660045
115.163753	4192.388091	23.665063
115.589906	4193.553574	23.670080
115.444145	4189.305920	23.675098
115.674857	4193.178185	23.680115
115.761683	4197.113992	23.685133
115.496240	4190.876606	23.690151
115.531696	4200.846274	23.695168
115.851362	4219.759419	23.700186
116.235479	4227.180077	23.705203
116.278398	4224.725703	23.710221
116.109182	4230.803892	23.715239
116.443636	4219.017984	23.720256
116.504442	4244.507600	23.725274
116.551664	4254.199759	23.730291
117.023035	4251.159213	23.735309
116.752061	4260.160622	23.740327
117.006395	4261.591519	23.745344
116.686713	4250.574722	23.750362
117.093625	4266.220644	23.755379
116.881471	4272.737849	23.760397
117.187209	4279.411615	23.765415
117.701584	4278.388437	23.770432
117.538447	4287.221644	23.775450
117.799934	4293.613742	23.780467
117.617800	4311.924064	23.785485
118.066896	4307.694230	23.790503
118.326999	4298.633246	23.795520
118.171145	4310.471277	23.800538
118.386637	4328.476144	23.805555
118.635108	4328.901678	23.810573
118.475671	4337.552799	23.815591
118.813460	4337.473399	23.820608
118.582591	4339.634108	23.825626
118.731000	4357.165821	23.830643
119.159541	4367.490739	23.835661
119.303521	4367.321705	23.840679
119.284059	4363.650795	23.845696
119.272752	4368.685975	23.850714
119.115835	4387.239079	23.855731
119.459729	4403.760157	23.860749
119.587914	4405.025683	23.865767
119.847136	4412.460768	23.870784
119.444508	4427.867376	23.875802
119.685494	4423.203768	23.880819
120.143224	4430.313135	23.885837
120.396625	4451.196653	23.890855
120.631428	4442.180320	23.895872
120.553618	4458.784917	23.900890
120.537084	4458.975097	23.905907
121.052490	4459.117540	23.910925
120.964761	4475.911993	23.915943
121.449415	4476.697343	23.920960
121.202979	4488.876082	23.925978
121.223198	4476.938745	23.930995
121.503267	4484.543657	23.936013
121.621969	4506.881465	23.941031
121.922777	4510.348508	23.946048
121.938630	4503.590475	23.951066
122.048216	4496.181494	23.956083
122.481678	4505.924561	23.961101
122.053953	4515.469760	23.966119
122.461131	4521.319348	23.971136
122.517855	4532.734213	23.976154
122.905332	4532.853699	23.981171
123.065573	4530.229489	23.986189
122.662716	4545.494117	23.991207
123.216267	4530.930686	23.996224
123.156175	4552.122059	24.001242
123.632959	4562.447798	24.006259
124.037668	4565.662239	24.011277
123.648208	4566.686917	24.016295
123.588024	4565.519279	24.021312
123.840439	4564.608665	24.026330
123.747672	4559.356430	24.031347
123.704928	4562.081391	24.036365
123.825516	4575.659865	24.041383
124.085356	4579.136448	24.046400
124.334597	4595.802118	24.051418
124.296380	4594.538322	24.056435
124.160831	4589.325432	24.061453
124.277035	4613.057582	24.066471
124.629423	4610.980776	24.071488
124.769159	4617.249416	24.076506
124.959795	4630.005687	24.081523
125.356006	4640.036506	24.086541
125.465256	4656.116281	24.091559
125.457708	4652.743746	24.096576
125.869611	4646.020610	24.101594
126.009130	4640.972106	24.106611
126.039377	4649.583395	24.111629
125.427026	4647.172658	24.116647
126.297514	4648.493906	24.121664
126.456741	4669.750386	24.126682
126.339354	4670.365919	24.131699
126.441167	4664.526346	24.136717
126.258666	4674.284286	24.141735
126.684967	4663.140782	24.146752
126.480994	4690.273398	24.151770
126.865654	4694.834175	24.156787
127.083383	4693.352478	24.161805
126.681753	4695.414278	24.166823
127.064921	4716.436956	24.171840
127.398194	4727.214891	24.176858
127.429866	4727.284898	24.181875
127.642306	4736.529951	24.186893
127.454693	4757.861580	24.191911
127.981262	4755.961499	24.196928
128.230276	4766.437222	24.201946
128.334767	4770.582474	24.206963
128.429914	4763.197013	24.211981
128.568949	4781.541830	24.216999
128.768360	4788.510569	24.222016
128.774482	4792.506715	24.227034
128.426679	4789.278962	24.232051
129.011296	4805.702419	24.237069
128.875642	4827.768915	24.242087
129.197593	4821.081829	24.247104
129.024813	4825.839879	24.252122
129.331276	4838.470089	24.257139
129.493749	4847.952615	24.262157
129.324194	4855.482780	24.267175
129.645447	4866.767952	24.272192
130.016340	4878.316998	24.277210
130.346256	4879.830747	24.282227
130.718767	4876.324887	24.287245
130.620261	4890.452867	24.292263
130.790567	4878.973136	24.297280
130.688154	4879.394062	24.302298
130.964662	4903.109222	24.307315
131.217878	4896.215729	24.312333
131.307872	4901.585549	24.317351
131.133952	4895.939887	24.322368
131.256717	4899.687242	24.327386
131.119867	4907.766006	24.332403
131.348578	4925.874112	24.337421
131.640922	4926.076651	24.342439
131.546599	4934.983111	24.347456
131.715065	4948.311854	24.352474
131.671717	4946.204717	24.357491
132.365543	4949.884105	24.362509
132.367935	4975.968866	24.367527
132.649705	4988.843454	24.372544
132.526335	4983.836310	24.377562
132.466556	4996.251945	24.382579
132.933611	4987.052422	24.387597
133.171287	4992.220298	24.392615
133.519885	5009.158599	24.397632
133.576455	5015.068670	24.402650
133.334441	5011.744249	24.407667
133.568038	5003.625504	24.412685
133.694475	5013.141253	24.417703
133.390032	5008.825098	24.422720
133.644086	5024.602169	24.427738
133.436321	5049.169681	24.432755
133.876995	5030.958777	24.437773
134.029930	5059.525702	24.442791
134.235580	5076.040413	24.447808
134.651717	5074.105389	24.452826
134.511721	5081.839851	24.457843
134.974356	5092.590759	24.462861
134.669499	5109.483585	24.467879
135.123025	5109.781552	24.472896
135.015661	5117.539776	24.477914
134.932415	5132.798624	24.482931
135.377174	5133.935123	24.487949
135.505879	5151.345384	24.492967
135.526992	5154.650501	24.497984
135.687573	5156.955319	24.503002
136.115070	5167.494743	24.508019
136.588964	5165.341090	24.513037
136.891290	5178.678229	24.518055
137.020424	5188.738966	24.523072
137.062994	5189.852546	24.528090
136.868742	5183.088775	24.533107
136.985741	5177.546924	24.538125
137.159657	5191.245481	24.543143
137.269366	5180.472850	24.548160
137.470728	5178.596533	24.553178
137.440386	5217.896991	24.558195
137.495135	5213.004056	24.563213
137.585147	5217.873935	24.568231
137.544534	5225.662132	24.573248
137.798791	5230.768680	24.578266
138.142649	5250.596098	24.583283
138.119021	5256.106086	24.588301
138.439086	5268.101264	24.593319
138.316853	5275.406467	24.598336
138.729891	5280.257245	24.603354
138.680186	5286.661405	24.608371
138.872807	5308.563695	24.613389
139.050847	5317.452931	24.618407
139.286621	5324.556467	24.623424
139.243999	5318.792490	24.628442
139.220473	5349.681067	24.633459
139.985526	5349.691320	24.638477
140.012104	5350.301597	24.643495
139.607776	5359.915101	24.648512
140.079052	5369.084294	24.653530
140.049923	5365.696272	24.658547
140.370316	5361.720127	24.663565
140.805576	5376.313950	24.668583
140.703270	5383.903735	24.673600
140.933497	5397.501820	24.678618
140.885871	5396.925414	24.683635
141.368543	5395.854648	24.688653
141.313687	5401.764377	24.693671
141.418676	5420.648304	24.698688
141.706855	5420.325105	24.703706
141.680355	5429.228908	24.708723
141.893645	5428.278250	24.713741
141.754052	5429.648743	24.718759
141.972599	5456.158086	24.723776
141.910816	5455.169010	24.728794
141.951495	5462.181604	24.733811
142.652877	5462.457525	24.738829
142.369453	5469.834339	24.743847
142.471589	5490.966316	24.748864
142.967485	5482.792958	24.753882
143.090647	5495.844977	24.758899
143.055945	5495.473541	24.763917
143.349688	5507.949685	24.768935
143.694259	5516.340992	24.773952
143.685941	5512.536853	24.778970
143.532257	5525.360988	24.783987
143.848484	5532.655680	24.789005
144.094673	5538.193634	24.794023
143.988351	5545.801486	24.799040
144.570111	5546.850412	24.804058
144.807084	5552.150102	24.809075
144.747374	5564.774468	24.814093
144.740421	5583.318385	24.819111
144.694795	5579.070341	24.824128
144.725520	5577.867524	24.829146
144.845506	5592.542386	24.834163
145.189014	5603.986247	24.839181
144.995545	5616.768993	24.844199
145.129732	5640.246945	24.849216
145.753612	5635.572476	24.854234
145.535280	5651.713703	24.859251
145.597790	5660.120587	24.864269
146.304208	5670.663089	24.869287
145.947506	5678.147395	24.874304
146.481110	5698.870916	24.879322
146.756057	5715.579210	24.884339
146.704483	5706.618133	24.889357
146.834189	5722.367237	24.894375
146.897533	5739.245182	24.899392
147.138593	5727.028244	24.904410
147.345688	5737.708816	24.909427
147.447247	5755.410885	24.914445
147.622212	5756.685331	24.919463
147.455274	5768.043160	24.924480
148.193701	5776.377404	24.929498
148.243816	5804.045236	24.934515
148.535306	5792.819259	24.939533
148.634494	5800.233020	24.944551
148.599525	5797.710550	24.949568
148.940766	5809.090360	24.954586
148.999064	5827.391469	24.959603
149.284456	5834.822912	24.964621
149.199734	5835.072807	24.969639
149.120018	5831.248494	24.974656
149.486808	5845.251627	24.979674
149.509849	5852.818959	24.984691
150.058093	5849.304324	24.989709
149.937195	5846.596017	24.994727
149.505671	5871.365983	24.999744
150.257576	5871.422121	25.004762
150.239012	5889.045751	25.009779
150.416051	5905.694430	25.014797
151.047397	5907.769192	25.019815
151.110941	5922.751763	25.024832
151.240790	5906.691498	25.029850
151.288623	5916.912614	25.034867
151.381830	5922.378331	25.039885
151.535024	5930.633349	25.044903
151.364702	5944.878490	25.049920
151.869532	5937.092454	25.054938
151.598211	5953.716041	25.059955
151.863398	5968.468066	25.064973
152.285899	5978.181581	25.069991
151.973324	5972.409993	25.075008
152.233661	5974.085370	25.080026
152.326392	6001.658307	25.085043
152.657908	6004.166144	25.090061
152.741009	5996.698617	25.095079
152.683516	6029.896841	25.100096
152.988963	6027.698063	25.105114
153.223603	6039.105105	25.110131
153.282704	6062.735881	25.115149
153.542845	6058.486012	25.120167
153.839773	6065.048206	25.125184
154.154518	6070.148974	25.130202
154.488651	6081.145061	25.135219
154.333715	6088.830904	25.140237
154.732463	6079.645577	25.145255
154.716746	6093.273880	25.150272
154.781896	6092.739452	25.155290
154.771432	6101.122011	25.160307
154.771235	6121.079440	25.165325
155.230332	6120.839816	25.170343
155.002750	6143.000528	25.175360
155.116942	6143.803872	25.180378
155.542237	6156.480485	25.185395
155.728273	6178.017699	25.190413
156.139466	6187.964746	25.195431
155.894061	6197.389483	25.200448
155.976542	6200.917394	25.205466
156.719646	6204.457429	25.210483
156.740069	6206.259889	25.215501
157.289335	6201.551121	25.220519
157.004659	6210.787835	25.225536
157.217912	6228.115233	25.230554
157.314292	6231.492012	25.235571
157.342459	6242.308022	25.240589
157.820470	6227.466092	25.245607
157.641125	6257.766750	25.250624
158.082108	6263.918550	25.255642
158.170071	6262.334509	25.260659
158.225228	6265.132973	25.265677
158.416416	6269.453305	25.270695
158.404197	6289.432623	25.275712
158.927044	6298.108331	25.280730
159.026511	6294.415742	25.285747
159.119171	6304.069769	25.290765
159.462744	6314.662820	25.295783
159.299829	6314.640950	25.300800
159.288440	6320.435950	25.305818
159.476818	6336.835929	25.310835
159.008476	6351.761494	25.315853
159.968058	6346.674598	25.320871
160.176786	6379.482664	25.325888
160.567935	6370.501609	25.330906
160.283090	6383.336695	25.335923
160.450254	6387.194022	25.340941
160.769149	6411.722714	25.345959
160.851628	6417.491215	25.350976
160.898643	6408.049589	25.355994
161.149763	6435.519938	25.361011
161.088178	6457.999394	25.366029
161.275263	6453.859145	25.371047
161.467391	6478.945201	25.376064
161.636262	6485.965029	25.381082
161.830999	6487.468593	25.386099
161.851174	6514.863047	25.391117
162.213431	6513.433695	25.396135
162.123660	6530.899700	25.401152
162.377869	6538.211805	25.406170
162.700890	6557.770651	25.411187
162.634264	6563.309466	25.416205
163.138745	6573.020832	25.421223
163.190852	6578.208478	25.426240
163.039268	6587.665984	25.431258
163.738871	6594.762765	25.436275
163.566842	6602.479246	25.441293
164.558969	6605.097753	25.446311
164.514507	6602.908673	25.451328
164.499858	6623.218009	25.456346
164.751575	6622.342444	25.461363
164.519111	6632.568599	25.466381
164.995516	6635.193570	25.471399
165.314472	6632.829456	25.476416
165.156491	6637.932127	25.481434
165.408353	6654.871656	25.486451
165.169820	6669.823341	25.491469
165.740890	6665.477832	25.496487
165.494232	6671.193703	25.501504
165.873972	6693.083155	25.506522
166.083310	6698.644936	25.511539
165.647633	6708.580246	25.516557
165.996511	6722.965543	25.521575
166.395705	6733.576463	25.526592
166.407342	6756.193094	25.531610
166.619606	6758.440389	25.536627
166.532282	6773.471145	25.541645
167.132443	6791.129800	25.546663
167.498531	6794.447961	25.551680
167.897458	6803.872915	25.556698
168.477687	6811.039135	25.561715
168.201135	6823.578662	25.566733
168.410096	6811.363039	25.571751
168.702314	6808.183471	25.576768
168.689602	6816.621123	25.581786
168.742886	6837.584210	25.586803
168.569450	6843.115569	25.591821
168.906051	6848.342141	25.596839
169.080530	6871.294307	25.601856
169.196085	6878.348322	25.606874
169.268777	6877.407029	25.611891
169.750202	6897.822980	25.616909
170.155824	6902.697152	25.621927
169.956302	6908.647101	25.626944
170.234006	6908.949356	25.631962
170.522149	6917.536606	25.636979
170.671575	6938.389433	25.641997
170.844635	6938.438057	25.647015
170.659226	6943.273650	25.652032
170.322669	6951.440407	25.657050
171.054890	6967.099082	25.662067
171.245294	6986.357474	25.667085
171.525655	6983.753965	25.672103
171.745545	7001.908063	25.677120
171.760300	7019.323474	25.682138
171.758214	7027.461783	25.687156
172.330558	7041.488334	25.692173
172.171427	7056.941547	25.697191
172.271628	7064.917274	25.702208
172.419370	7080.665548	25.707226
172.944187	7093.287886	25.712244
172.681918	7104.285576	25.717261
172.945892	7114.225247	25.722279
173.450612	7134.157238	25.727296
173.596495	7139.635153	25.732314
173.743973	7140.620491	25.737332
173.845891	7168.980740	25.742349
174.249130	7169.819862	25.747367
174.173721	7173.018097	25.752384
174.455600	7179.135117	25.757402
174.911281	7183.674262	25.762420
174.633981	7193.501799	25.767437
175.185652	7186.354801	25.772455
175.287555	7191.276884	25.777472
175.016148	7208.133352	25.782490
175.166378	7224.583877	25.787508
175.216802	7229.934256	25.792525
175.713814	7251.819286	25.797543
175.834608	7256.847742	25.802560
175.660781	7259.608611	25.807578
176.000107	7279.402722	25.812596
176.011225	7294.029431	25.817613
176.547060	7304.659116	25.822631
177.024659	7317.178387	25.827648
176.842973	7322.427747	25.832666
177.503779	7333.490450	25.837684
177.280893	7346.895741	25.842701
177.362559	7344.492759	25.847719
177.822698	7360.806374	25.852736
177.580622	7380.780948	25.857754
178.426542	7380.638066	25.862772
178.302792	7398.659593	25.867789
178.695971	7408.052783	25.872807
178.783646	7405.805529	25.877824
178.663790	7411.541669	25.882842
179.025122	7429.765825	25.887860
178.690053	7441.079785	25.892877
179.093749	7465.664630	25.897895
179.365524	7465.874942	25.902912
179.258123	7475.244557	25.907930
179.881866	7497.946197	25.912948
180.096426	7506.636500	25.917965
180.202880	7517.755486	25.922983
180.763471	7538.781387	25.928000
180.589190	7538.072247	25.933018
181.188350	7545.356180	25.938036
181.132545	7564.655959	25.943053
180.980459	7570.379366	25.948071
181.188801	7570.457607	25.953088
181.106424	7601.127593	25.958106
181.342134	7602.835572	25.963124
181.709932	7620.689498	25.968141
182.007109	7634.454095	25.973159
182.705854	7631.321397	25.978176
182.787249	7651.040453	25.983194
183.222424	7665.776225	25.988212
183.209543	7662.176703	25.993229
183.474518	7649.876356	25.998247
183.605948	7651.248727	26.003264
183.385813	7657.919076	26.008282
183.845856	7675.519969	26.013300
183.737257	7684.785155	26.018317
184.121961	7682.300549	26.023335
183.846288	7697.141200	26.028352
184.145826	7730.956231	26.033370
184.305122	7722.831040	26.038388
184.383510	7757.163892	26.043405
184.414336	7761.565478	26.048423
184.895874	7770.225991	26.053440
184.899109	7790.574042	26.058458
185.329638	7797.672514	26.063476
185.434704	7821.434589	26.068493
185.664781	7835.836595	26.073511
186.148626	7834.463438	26.078528
186.143047	7850.766298	26.083546
186.676845	7854.956425	26.088564
186.409694	7858.633840	26.093581
186.437322	7880.012106	26.098599
186.533004	7876.332376	26.103616
186.917529	7885.461070	26.108634
186.932621	7902.210293	26.113652
187.019382	7912.048218	26.118669
187.016432	7928.678370	26.123687
187.534847	7947.080374	26.128704
187.746015	7959.968676	26.133722
187.926445	7976.971838	26.138740
188.253433	7980.701548	26.143757
188.159726	8000.760292	26.148775
188.510610	8015.214175	26.153792
188.796243	8020.149479	26.158810
188.964144	8032.193575	26.163828
189.144974	8050.029260	26.168845
189.306209	8062.754983	26.173863
189.848445	8078.758058	26.178880
189.731979	8093.233310	26.183898
190.186362	8089.109118	26.188916
190.286753	8106.551746	26.193933
190.312376	8115.326372	26.198951
190.415873	8116.728603	26.203968
190.447153	8135.288502	26.208986
191.166587	8147.633007	26.214004
191.020597	8170.924345	26.219021
191.191665	8178.970839	26.224039
191.762268	8178.501690	26.229056
191.341056	8204.727557	26.234074
191.865034	8215.041618	26.239092
192.532930	8222.957214	26.244109
192.514546	8233.442025	26.249127
193.082952	8236.465576	26.254144
192.759988	8252.862246	26.259162
193.452785	8256.095235	26.264180
193.616601	8268.110257	26.269197
193.243858	8267.184195	26.274215
193.707795	8263.764096	26.279232
194.063942	8290.853290	26.284250
193.967512	8304.817403	26.289268
193.966982	8306.607025	26.294285
194.199391	8313.983419	26.299303
194.534251	8323.363951	26.304320
194.712950	8338.371142	26.309338
194.938646	8342.670592	26.314356
195.094798	8358.957492	26.319373
195.148861	8372.370660	26.324391
195.410300	8384.292452	26.329408
195.274200	8398.340390	26.334426
195.463422	8420.071537	26.339444
196.033808	8439.587911	26.344461
195.886408	8452.079817	26.349479
196.191586	8466.531426	26.354496
196.046476	8486.886766	26.359514
196.695462	8497.459183	26.364532
197.050987	8505.228048	26.369549
197.074936	8521.809482	26.374567
197.299977	8531.895106	26.379584
197.357800	8553.181075	26.384602
197.625426	8559.404957	26.389620
197.931149	8566.330638	26.394637
198.198702	8588.789460	26.399655
198.425807	8597.346754	26.404672
198.609506	8619.630439	26.409690
199.182039	8611.804348	26.414708
199.543025	8608.594947	26.419725
199.377826	8631.129268	26.424743
199.771890	8634.311665	26.429760
199.852391	8656.358042	26.434778
199.855724	8656.445746	26.439796
200.210423	8641.053257	26.444813
200.293051	8680.311779	26.449831
200.469684	8684.251598	26.454848
200.317725	8684.330303	26.459866
200.509058	8699.041955	26.464884
201.040656	8709.508674	26.469901
200.979506	8715.189113	26.474919
201.580244	8728.334249	26.479936
201.590521	8739.292764	26.484954
201.828062	8738.109883	26.489972
201.889244	8751.756916	26.494989
202.107486	8774.229661	26.500007
202.170064	8781.928917	26.505024
202.471733	8809.377718	26.510042
202.620846	8815.109306	26.515060
202.813558	8829.492399	26.520077
202.399791	8850.943327	26.525095
202.909149	8850.098330	26.530112
202.997550	8877.420227	26.535130
203.519087	8895.001293	26.540148
203.719304	8898.333921	26.545165
203.508104	8929.899700	26.550183
204.094881	8937.714063	26.555200
204.451666	8959.880622	26.560218
204.788605	8974.445596	26.565236
204.779723	8990.965993	26.570253
204.950566	8995.065954	26.575271
205.300511	9017.542488	26.580288
205.647690	9042.295869	26.585306
205.694517	9046.405307	26.590324
205.878520	9066.006774	26.595341
206.022132	9085.985931	26.600359
206.492342	9090.516144	26.605376
206.932462	9104.879876	26.610394
206.883488	9120.363369	26.615412
207.414578	9128.917986	26.620429
207.278901	9141.992948	26.625447
207.990653	9144.696829	26.630464
208.301249	9165.820553	26.635482
208.138455	9165.541871	26.640500
208.491786	9172.203172	26.645517
208.159814	9179.854384	26.650535
208.464802	9204.366084	26.655552
208.804372	9208.891136	26.660570
209.002306	9219.044691	26.665588
209.513964	9233.584975	26.670605
209.508126	9239.106015	26.675623
209.519758	9259.027641	26.680640
209.339199	9270.338636	26.685658
209.594766	9293.266741	26.690676
210.027293	9301.586467	26.695693
210.245267	9327.036681	26.700711
210.401781	9335.454803	26.705728
210.550927	9352.642626	26.710746
210.454911	9367.242474	26.715764
211.113134	9386.735265	26.720781
211.136010	9393.771846	26.725799
211.455448	9406.296855	26.730816
212.028234	9443.174660	26.735834
212.138400	9443.594450	26.740852
212.888035	9455.822354	26.745869
212.828390	9462.248750	26.750887
212.748013	9465.924030	26.755904
213.337701	9484.863493	26.760922
213.102790	9487.041707	26.765940
213.595890	9497.151398	26.770957
213.831966	9512.265222	26.775975
214.314297	9514.907038	26.780992
214.352580	9530.848340	26.786010
214.445247	9513.401470	26.791028
214.755519	9535.514291	26.796045
214.961967	9552.416382	26.801063
215.011930	9543.956229	26.806080
215.088077	9554.732705	26.811098
215.075336	9581.729089	26.816116
215.436891	9589.841715	26.821133
215.299891	9602.676239	26.826151
215.531633	9625.157409	26.831168
215.913744	9637.249254	26.836186
216.280452	9664.539124	26.841204
216.256497	9663.186704	26.846221
216.249814	9696.171148	26.851239
216.759029	9712.212843	26.856256
216.855273	9714.731010	26.861274
217.070728	9747.685949	26.866292
217.477154	9755.829843	26.871309
217.682071	9776.174684	26.876327
217.635034	9788.880276	26.881344
218.110972	9810.485608	26.886362
218.089353	9834.329916	26.891380
218.409966	9845.415939	26.896397
218.718370	9865.102602	26.901415
219.494773	9873.219300	26.906432
219.399020	9880.389913	26.911450
219.636710	9905.204477	26.916468
220.269591	9910.784063	26.921485
220.529028	9917.497426	26.926503
220.487856	9939.675964	26.931520
220.495774	9951.656577	26.936538
220.771392	9963.070715	26.941556
221.175833	9966.893656	26.946573
221.237165	9986.870208	26.951591
221.017084	9994.182722	26.956608
221.219466	10016.938694	26.961626
221.468624	10037.792513	26.966644
221.867529	10049.844875	26.971661
222.088540	10072.474965	26.976679
221.929917	10085.493835	26.981696
222.622860	10111.682905	26.986714
222.874724	10125.246833	26.991732
223.347567	10140.868814	26.996749
223.133520	10152.605821	27.001767
223.494644	10167.626349	27.006784
224.241310	10181.079427	27.011802
224.002731	10199.170361	27.016820
224.569482	10203.590420	27.021837
224.583728	10225.620771	27.026855
225.020752	10248.421805	27.031872
224.884984	10249.799952	27.036890
224.794580	10268.178422	27.041908
225.261599	10283.852707	27.046925
225.598828	10299.320010	27.051943
225.661458	10312.543555	27.056960
225.957464	10329.961816	27.061978
225.911547	10363.000595	27.066996
226.379576	10373.316648	27.072013
226.700294	10388.899412	27.077031
227.143570	10392.975993	27.082048
227.506688	10409.778273	27.087066
227.108964	10426.788203	27.092084
227.693463	10437.702639	27.097101
227.896414	10447.474097	27.102119
228.112523	10478.184599	27.107136
228.377637	10478.551246	27.112154
228.449648	10500.394403	27.117172
229.097667	10506.878389	27.122189
228.635017	10514.005135	27.127207
229.100224	10541.062815	27.132224
229.279875	10538.880275	27.137242
229.629637	10572.414196	27.142260
229.657876	10580.909313	27.147277
229.681818	10600.703752	27.152295
230.114119	10612.959775	27.157312
230.560248	10630.451241	27.162330
230.748458	10651.387617	27.167348
230.975906	10662.847239	27.172365
231.396035	10682.054832	27.177383
231.342682	10685.325750	27.182400
231.594182	10698.664142	27.187418
231.892107	10721.971725	27.192436
232.255641	10744.546922	27.197453
232.598508	10748.143114	27.202471
232.601652	10788.113966	27.207488
232.759795	10777.651725	27.212506
232.930348	10804.748294	27.217524
233.191726	10816.375727	27.222541
233.414114	10836.466163	27.227559
233.881145	10847.847735	27.232576
234.077601	10867.153951	27.237594
234.214948	10880.698054	27.242612
234.418131	10902.426344	27.247629
234.947786	10910.735596	27.252647
235.018386	10919.235710	27.257664
235.397340	10941.927590	27.262682
235.563100	10959.846228	27.267700
236.237420	10965.003406	27.272717
236.002205	10980.208305	27.277735
236.110437	10993.480021	27.282752
236.420882	10994.638772	27.287770
236.787150	11029.693672	27.292788
236.799152	11032.134586	27.297805
237.130951	11066.086087	27.302823
237.375992	11075.014367	27.307840
237.816858	11085.819848	27.312858
237.648617	11104.608383	27.317876
238.152420	11132.144378	27.322893
238.340198	11148.799946	27.327911
238.433639	11166.602357	27.332928
238.737703	11187.815707	27.337946
238.897444	11207.352914	27.342964
239.183851	11221.789647	27.347981
239.657620	11233.366537	27.352999
239.732783	11249.004891	27.358016
240.544300	11266.502859	27.363034
240.606501	11285.656087	27.368052
240.704191	11299.737271	27.373069
241.106852	11312.877102	27.378087
241.124910	11326.103334	27.383104
241.542209	11335.108862	27.388122
241.625852	11349.876992	27.393140
241.850869	11369.994448	27.398157
242.192000	11366.829539	27.403175
242.413783	11384.501486	27.408192
242.571658	11413.899141	27.413210
242.578204	11416.943671	27.418228
242.932909	11436.007786	27.423245
242.996407	11446.489844	27.428263
243.237250	11468.019672	27.433280
244.174545	11464.067721	27.438298
244.232226	11485.600262	27.443316
244.807476	11487.148583	27.448333
245.166075	11493.613043	27.453351
245.226952	11496.891250	27.458368
245.409524	11504.680709	27.463386
245.563814	11523.547219	27.468404
245.561841	11519.699233	27.473421
245.704761	11525.294171	27.478439
245.727281	11555.552657	27.483456
245.860832	11559.215916	27.488474
246.244518	11578.131247	27.493492
246.343770	11590.331181	27.498509
246.470168	11604.034475	27.503527
246.267203	11638.697110	27.508544
247.108096	11655.326441	27.513562
247.236671	11680.743180	27.518580
247.552051	11706.231509	27.523597
247.809582	11714.302535	27.528615
247.966370	11735.455072	27.533632
247.965992	11756.018332	27.538650
248.548018	11779.256094	27.543668
248.706983	11805.414057	27.548685
248.836527	11817.707634	27.553703
249.072354	11839.984052	27.558720
249.400169	11863.883938	27.563738
249.654944	11892.900918	27.568756
250.070013	11902.604345	27.573773
250.243086	11931.502542	27.578791
250.982933	11951.321384	27.583808
251.387918	11959.862129	27.588826
251.775838	11967.591888	27.593844
252.037888	11986.071654	27.598861
252.434818	11996.120833	27.603879
252.516547	12002.142012	27.608896
252.538066	12014.917610	27.613914
252.549859	12025.502338	27.618932
252.931660	12054.642794	27.623949
253.040136	12059.899334	27.628967
253.378438	12080.217976	27.633984
253.621082	12093.933208	27.639002
253.771313	12125.828445	27.644020
254.414454	12130.593310	27.649037
254.686817	12140.641101	27.654055
254.776007	12161.866818	27.659072
255.233998	12160.051681	27.664090
254.947981	12188.473927	27.669108
255.081251	12199.760344	27.674125
255.731601	12227.944447	27.679143
255.904275	12247.234982	27.684160
256.377157	12259.271277	27.689178
256.463343	12278.343729	27.694196
257.018721	12297.130700	27.699213
257.017092	12313.521759	27.704231
257.274467	12322.810311	27.709248
257.669531	12336.823577	27.714266
257.862467	12358.474384	27.719284
257.994411	12369.857256	27.724301
258.105450	12386.087964	27.729319
258.202626	12416.934486	27.734336
258.528574	12427.722045	27.739354
258.838390	12455.609072	27.744372
259.358609	12467.955200	27.749389
259.601968	12495.292337	27.754407
259.597635	12511.947181	27.759424
259.560581	12526.279386	27.764442
259.527421	12548.604376	27.769460
259.871236	12575.921901	27.774477
260.490213	12599.291042	27.779495
260.887388	12627.684697	27.784512
260.941220	12631.745840	27.789530
261.696232	12667.307334	27.794548
261.449002	12671.758576	27.799565
262.095114	12694.904352	27.804583
262.609555	12718.896004	27.809600
262.662440	12726.948564	27.814618
262.867339	12741.820842	27.819636
262.919007	12766.089135	27.824653
263.665222	12765.327729	27.829671
263.265404	12786.979350	27.834688
263.580547	12805.051057	27.839706
263.757981	12825.288494	27.844724
264.066315	12851.922190	27.849741
264.772001	12865.946051	27.854759
264.773673	12888.673865	27.859776
265.272777	12908.929171	27.864794
265.488679	12919.272769	27.869812
265.687966	12938.342285	27.874829
266.396787	12953.534887	27.879847
266.509288	12984.487110	27.884864
266.714127	12985.245894	27.889882
267.048875	13004.126081	27.894900
267.536447	13017.109891	27.899917
267.816588	13037.125782	27.904935
267.750285	13043.710706	27.909952
267.991546	13062.269201	27.914970
268.290653	13075.906609	27.919988
268.515308	13100.622695	27.925005
268.663046	13123.381858	27.930023
268.601875	13135.766252	27.935040
268.900629	13150.579281	27.940058
269.110357	13176.832717	27.945076
269.461161	13198.542084	27.950093
270.161166	13205.079257	27.955111
270.332715	13248.138119	27.960128
270.442519	13256.192569	27.965146
270.995764	13279.562528	27.970164
271.031234	13303.464002	27.975181
271.577998	13322.763351	27.980199
271.793957	13348.365251	27.985216
271.779635	13360.991047	27.990234
272.149442	13374.678481	27.995252
272.246124	13393.992396	28.000269
273.227430	13416.874256	28.005287
273.125407	13444.998065	28.010304
273.781154	13455.212611	28.015322
274.447712	13457.037568	28.020340
274.245146	13482.103730	28.025357
274.400490	13497.820050	28.030375
274.588355	13515.209210	28.035392
274.761118	13521.620890	28.040410
275.013353	13545.288362	28.045428
275.432431	13568.499691	28.050445
275.836395	13582.830880	28.055463
275.860514	13592.152399	28.060480
276.110374	13616.705956	28.065498
276.112884	13642.159218	28.070516
276.095979	13653.747226	28.075533
276.681678	13680.517678	28.080551
277.107022	13718.198664	28.085568
277.370605	13725.635444	28.090586
277.911291	13751.620827	28.095604
277.439075	13777.507286	28.100621
277.887822	13790.431951	28.105639
278.175151	13814.437542	28.110656
277.826820	13866.627468	28.115674
278.749885	13882.138534	28.120692
278.962982	13915.605089	28.125709
279.670129	13940.450751	28.130727
279.711675	13961.378629	28.135744
280.144155	13987.142744	28.140762
280.538237	14002.569556	28.145780
280.427264	14025.402668	28.150797
280.768741	14034.930445	28.155815
281.264599	14057.781534	28.160832
281.521773	14076.058067	28.165850
281.934776	14093.167974	28.170868
282.075334	14116.605749	28.175885
282.209193	14125.277536	28.180903
282.614170	14165.570928	28.185920
282.592534	14170.272108	28.190938
283.016411	14181.931072	28.195956
282.904678	14217.092361	28.200973
283.483654	14242.908320	28.205991
284.016454	14270.651329	28.211008
284.083133	14293.750151	28.216026
284.692012	14317.547354	28.221044
284.675190	14338.433358	28.226061
285.039681	14358.622899	28.231079
285.157389	14389.854294	28.236096
285.507826	14423.034461	28.241114
286.058046	14435.734865	28.246132
286.049123	14468.928795	28.251149
286.317005	14491.756702	28.256167
286.678824	14518.077008	28.261184
286.849697	14536.796954	28.266202
287.473350	14559.468475	28.271220
287.628677	14588.646976	28.276237
287.961868	14600.210912	28.281255
288.488657	14637.722837	28.286272
288.626929	14662.876337	28.291290
289.187446	14677.081775	28.296308
289.671493	14712.597983	28.301325
289.594549	14716.766353	28.306343
289.899539	14744.710126	28.311360
289.813393	14766.175453	28.316378
290.446338	14787.562980	28.321396
290.551358	14820.294398	28.326413
290.703274	14838.036037	28.331431
291.086591	14857.994583	28.336448
291.104911	14901.021682	28.341466
291.754598	14921.167956	28.346484
292.029101	14947.875298	28.351501
291.937203	14969.108607	28.356519
292.330502	15007.488128	28.361536
292.894594	15039.455467	28.366554
293.185150	15055.579607	28.371572
293.425366	15089.516874	28.376589
293.769207	15115.469198	28.381607
294.165725	15141.631916	28.386624
294.344874	15157.249777	28.391642
294.822217	15188.412256	28.396660
295.163278	15212.354302	28.401677
295.580705	15235.272013	28.406695
295.761248	15251.654065	28.411712
295.754981	15284.658527	28.416730
296.731190	15292.000359	28.421748
297.118328	15323.920271	28.426765
297.303918	15332.179136	28.431783
297.709971	15345.985173	28.436800
298.116206	15362.870601	28.441818
298.676590	15377.486423	28.446836
298.850392	15400.573844	28.451853
298.858572	15397.313455	28.456871
299.204410	15419.778347	28.461888
299.270231	15438.918554	28.466906
299.407790	15446.958475	28.471924
299.446511	15472.656041	28.476941
299.878541	15490.238643	28.481959
300.229779	15516.185656	28.486976
300.510818	15533.172319	28.491994
300.803949	15543.337782	28.497012
301.066353	15571.468092	28.502029
301.464414	15595.960755	28.507047
301.600321	15603.151575	28.512064
301.289083	15640.763285	28.517082
301.724346	15661.280010	28.522100
301.933162	15687.547109	28.527117
302.551750	15718.619500	28.532135
302.706560	15749.245343	28.537152
303.247823	15770.334113	28.542170
303.549423	15791.635864	28.547188
303.954266	15828.223505	28.552205
304.080601	15849.762318	28.557223
304.432764	15883.427429	28.562240
304.640329	15902.171249	28.567258
305.168243	15914.422608	28.572276
305.502463	15947.964736	28.577293
305.884451	15969.830258	28.582311
306.207190	15995.371402	28.587328
306.283351	16035.747383	28.592346
306.772320	16049.031265	28.597364
306.957246	16072.051604	28.602381
307.445868	16094.968218	28.607399
308.109474	16117.127832	28.612416
308.349070	16139.740500	28.617434
308.483409	16165.450150	28.622452
308.926476	16195.099347	28.627469
309.099523	16199.061310	28.632487
309.486715	16227.911293	28.637504
309.619559	16252.213926	28.642522
309.926098	16271.162463	28.647540
310.379314	16295.984335	28.652557
310.465325	16323.676997	28.657575
310.467765	16338.538735	28.662592
310.808022	16378.764759	28.667610
311.166240	16410.467772	28.672628
311.669321	16425.874149	28.677645
312.021694	16460.845386	28.682663
312.494905	16485.092134	28.687680
312.783569	16502.218814	28.692698
313.581911	16530.648368	28.697716
313.445153	16549.708288	28.702733
313.818549	16573.440523	28.707751
314.303651	16591.819339	28.712768
314.240283	16626.199239	28.717786
314.679053	16640.658190	28.722804
314.958325	16667.868748	28.727821
315.214618	16691.076752	28.732839
315.566113	16716.050033	28.737856
316.121007	16741.152087	28.742874
316.905768	16758.074142	28.747892
316.781647	16780.029087	28.752909
316.860696	16798.308153	28.757927
317.594524	16832.342434	28.762944
317.534167	16860.241432	28.767962
317.829876	16861.436156	28.772980
318.112565	16904.883489	28.777997
318.409797	16924.860360	28.783015
318.809881	16939.483578	28.788032
318.670397	16981.199371	28.793050
319.329742	16999.820951	28.798068
319.643547	17026.000350	28.803085
320.095421	17050.659672	28.808103
320.371507	17076.162925	28.813120
320.881614	17101.893921	28.818138
321.222281	17114.057332	28.823156
321.171003	17146.570195	28.828173
321.224965	17169.954154	28.833191
321.653403	17186.837800	28.838208
321.722582	17219.915651	28.843226
322.018412	17245.222041	28.848244
322.290698	17267.061710	28.853261
322.985024	17303.953147	28.858279
323.344806	17335.566273	28.863296
323.528513	17372.124543	28.868314
323.787294	17385.195358	28.873332
324.081599	17416.012469	28.878349
324.303790	17463.756821	28.883367
325.086629	17478.219565	28.888384
325.396532	17502.821061	28.893402
325.606355	17541.350316	28.898420
325.781875	17570.508729	28.903437
326.301119	17588.332942	28.908455
327.072722	17605.138261	28.913472
327.619798	17631.442432	28.918490
327.888398	17659.680904	28.923508
328.346831	17666.130561	28.928525
328.248318	17694.804871	28.933543
328.651284	17707.975065	28.938560
328.520729	17742.541773	28.943578
329.181182	17765.455979	28.948596
329.166704	17783.267701	28.953613
329.193840	17813.913757	28.958631
329.848788	17841.658416	28.963648
330.150824	17884.744190	28.968666
330.775133	17905.717965	28.973684
331.041048	17944.582506	28.978701
331.082777	17971.331656	28.983719
331.874967	17980.621782	28.988736
332.162162	18027.348257	28.993754
332.554445	18057.198352	28.998772
332.729196	18071.557172	29.003789
333.014951	18110.403065	29.008807
333.449643	18129.360946	29.013824
333.834146	18151.033509	29.018842
333.962763	18178.419617	29.023860
334.466813	18206.364781	29.028877
334.419701	18240.231510	29.033895
334.876745	18264.630145	29.038912
335.204069	18306.641006	29.043930
335.122145	18333.819414	29.048948
335.649316	18365.242933	29.053965
336.122289	18412.004430	29.058983
336.419094	18427.248160	29.064000
336.459785	18472.347372	29.069018
337.171398	18505.507664	29.074036
337.623601	18531.822641	29.079053
337.665483	18576.236268	29.084071
338.008318	18607.057044	29.089088
338.345966	18632.956058	29.094106
338.609984	18671.042370	29.099124
339.229518	18706.650460	29.104141
339.652935	18735.048042	29.109159
340.277735	18763.004149	29.114176
340.604785	18801.772335	29.119194
340.936741	18818.889546	29.124212
341.390294	18862.506112	29.129229
341.236698	18885.638327	29.134247
341.775782	18900.159935	29.139264
341.797731	18937.711504	29.144282
342.118652	18979.381499	29.149300
342.831072	19001.451826	29.154317
342.848300	19030.021053	29.159335
343.405368	19059.483186	29.164352
343.791662	19087.904846	29.169370
344.568918	19087.964061	29.174388
345.047965	19119.332336	29.179405
345.097099	19160.432924	29.184423
345.551145	19161.781365	29.189440
346.473195	19165.992320	29.194458
347.163603	19168.397254	29.199476
347.664147	19180.149585	29.204493
347.698662	19197.385684	29.209511
347.968421	19211.138679	29.214528
348.240210	19216.864725	29.219546
348.336362	19242.010123	29.224564
348.706196	19251.291931	29.229581
348.792550	19279.459241	29.234599
348.783315	19290.444650	29.239616
348.974873	19313.239854	29.244634
349.178102	19343.117197	29.249652
349.478828	19361.721882	29.254669
349.758282	19409.683077	29.259687
349.934345	19441.737280	29.264704
350.036929	19477.750851	29.269722
350.443321	19520.323941	29.274740
350.800019	19557.824765	29.279757
350.797876	19600.566437	29.284775
351.321133	19640.235796	29.289792
351.708841	19683.323131	29.294810
352.420002	19727.019218	29.299828
352.759274	19757.215326	29.304845
352.920921	19798.494374	29.309863
353.372454	19848.900165	29.314880
353.715159	19894.511385	29.319898
354.102095	19923.596452	29.324916
354.511422	19966.055122	29.329933
354.832488	19998.597194	29.334951
355.339404	20045.151181	29.339968
355.818500	20079.052958	29.344986
356.128601	20102.007793	29.350004
356.606401	20131.325708	29.355021
356.987165	20179.360664	29.360039
357.301389	20205.180877	29.365056
357.582243	20236.982837	29.370074
358.183020	20271.722476	29.375092
358.892757	20295.410804	29.380109
359.227246	20340.704589	29.385127
359.888747	20362.383154	29.390144
360.171881	20395.531311	29.395162
360.118386	20412.378064	29.400180
360.843951	20441.018715	29.405197
361.038943	20474.771178	29.410215
361.212516	20493.361877	29.415232
361.567622	20529.796326	29.420250
361.946682	20556.624756	29.425268
362.560892	20583.020270	29.430285
362.845156	20613.504474	29.435303
363.453307	20635.983589	29.440320
363.909289	20665.633953	29.445338
363.551867	20697.474446	29.450356
364.152345	20715.123086	29.455373
364.517973	20753.682933	29.460391
364.953094	20786.822524	29.465408
365.018006	20816.495195	29.470426
365.442255	20854.285731	29.475444
365.914665	20881.904841	29.480461
365.870221	20921.469246	29.485479
366.349813	20957.064293	29.490496
366.802283	20990.931335	29.495514
366.976613	21026.280577	29.500532
367.631116	21057.812703	29.505549
367.507343	21097.884072	29.510567
368.223722	21123.714943	29.515584
368.621629	21153.970109	29.520602
368.651636	21187.473801	29.525620
369.129526	21211.280559	29.530637
369.329792	21257.354150	29.535655
369.825055	21290.155312	29.540672
370.631349	21317.994301	29.545690
370.810947	21357.992528	29.550708
371.402822	21384.244808	29.555725
371.488582	21421.963269	29.560743
371.549692	21453.086525	29.565760
372.119398	21483.209854	29.570778
372.366238	21527.756716	29.575796
373.043880	21560.698547	29.580813
373.490194	21604.559972	29.585831
373.695451	21633.173537	29.590848
374.210032	21674.599137	29.595866
374.378226	21703.439662	29.600884
375.005660	21723.136015	29.605901
375.651723	21770.701317	29.610919
375.599781	21790.301874	29.615936
376.256863	21823.573967	29.620954
376.373446	21857.744195	29.625972
377.026266	21896.998644	29.630989
377.430367	21934.042921	29.636007
377.099550	21955.094469	29.641024
377.651529	21992.609491	29.646042
377.998737	22039.312084	29.651060
378.641478	22072.911818	29.656077
378.847367	22113.043088	29.661095
379.435007	22150.711809	29.666112
379.924967	22185.043323	29.671130
380.269909	22222.082242	29.676148
381.032914	22258.219732	29.681165
381.368799	22289.168287	29.686183
381.554068	22305.253833	29.691200
382.098930	22340.631348	29.696218
382.026741	22379.721327	29.701236
382.546627	22414.909200	29.706253
382.735264	22451.462043	29.711271
383.165244	22484.159657	29.716288
383.727475	22530.304652	29.721306
384.041453	22572.561805	29.726324
384.484949	22608.596744	29.731341
384.939928	22648.968785	29.736359
385.232622	22687.040601	29.741376
385.776367	22713.263498	29.746394
385.819956	22755.281979	29.751412
386.587204	22797.655595	29.756429
386.573456	22826.506029	29.761447
386.771925	22875.499596	29.766464
387.355485	22903.253460	29.771482
387.728175	22947.018608	29.776500
388.561889	22990.663563	29.781517
389.111128	23023.921164	29.786535
389.174723	23059.124271	29.791552
389.728513	23100.512221	29.796570
389.607003	23133.779935	29.801588
390.257221	23170.347957	29.806605
390.619700	23211.056693	29.811623
390.658037	23254.004380	29.816640
391.428450	23287.623294	29.821658
391.312042	23336.492047	29.826676
391.668770	23375.529243	29.831693
392.353750	23427.364112	29.836711
392.523425	23467.257043	29.841728
393.337421	23496.545808	29.846746
393.611141	23547.408346	29.851764
394.219022	23573.510040	29.856781
395.020140	23591.158529	29.861799
395.610435	23627.292803	29.866816
396.159710	23630.488020	29.871834
396.835679	23658.924781	29.876852
397.555612	23663.748965	29.881869
397.608124	23689.538938	29.886887
397.526431	23714.572208	29.891904
398.035107	23738.853641	29.896922
398.062702	23760.523073	29.901940
398.333887	23794.141898	29.906957
398.710379	23821.319702	29.911975
398.822760	23868.438266	29.916992
399.290151	23905.733434	29.922010
399.486625	23944.829953	29.927028
399.943599	23987.361880	29.932045
400.296102	24028.517305	29.937063
400.446481	24077.361467	29.942080
400.604120	24113.927758	29.947098
401.063929	24166.554214	29.952116
401.620486	24206.211529	29.957133
401.893767	24247.533521	29.962151
401.854182	24300.507790	29.967168
402.492031	24357.971426	29.972186
402.967334	24406.948925	29.977204
403.233159	24457.014479	29.982221
404.315334	24511.760924	29.987239
404.794021	24570.963998	29.992256
405.279354	24587.654954	29.997274
405.484876	24637.190150	30.002292
405.911780	24690.785533	30.007309
406.530722	24724.336140	30.012327
406.763661	24772.291941	30.017344
407.468763	24808.124362	30.022362
407.634135	24848.970513	30.027380
408.205196	24884.110924	30.032397
408.710269	24937.878665	30.037415
408.942186	24975.240312	30.042432
409.343906	25009.467571	30.047450
409.769332	25067.397605	30.052468
409.814174	25099.861139	30.057485
410.235093	25152.793526	30.062503
410.622278	25192.425933	30.067520
411.424823	25238.565424	30.072538
411.853862	25290.710033	30.077556
412.335388	25323.111318	30.082573
413.322106	25361.623255	30.087591
413.574439	25402.270294	30.092608
414.108482	25428.795464	30.097626
414.943724	25467.618083	30.102644
414.971787	25482.191982	30.107661
415.429157	25520.197228	30.112679
415.748546	25564.585047	30.117696
416.218863	25581.539653	30.122714
416.420548	25632.917062	30.127732
416.454727	25680.581830	30.132749
417.071185	25705.491660	30.137767
417.335724	25751.309837	30.142784
417.790812	25792.145081	30.147802
418.114106	25838.616099	30.152820
418.504768	25881.321411	30.157837
418.997763	25925.148482	30.162855
419.244789	25977.206985	30.167872
419.978231	25994.003420	30.172890
420.066919	26038.525196	30.177908
420.517360	26075.544071	30.182925
421.311056	26106.394011	30.187943
421.427895	26152.384318	30.192960
422.061590	26190.048112	30.197978
422.279503	26230.597151	30.202996
422.706103	26260.747907	30.208013
423.022019	26307.065296	30.213031
423.292118	26343.518443	30.218048
424.158498	26378.236253	30.223066
424.264439	26427.313690	30.228084
424.103023	26468.581982	30.233101
424.747009	26511.291177	30.238119
425.429148	26566.853083	30.243136
425.833256	26606.157958	30.248154
426.145383	26649.594124	30.253172
426.669817	26701.773015	30.258189
427.360688	26733.726062	30.263207
427.408144	26790.055884	30.268224
427.771096	26831.301509	30.273242
428.294506	26884.080395	30.278260
428.515953	26931.118432	30.283277
429.195699	26966.672558	30.288295
429.591862	27026.664221	30.293312
430.148687	27074.543015	30.298330
430.234186	27120.231991	30.303348
430.720099	27177.884774	30.308365
430.807891	27208.749223	30.313383
430.958026	27285.351087	30.318400
431.800994	27336.264943	30.323418
432.418362	27388.979393	30.328436
432.730893	27443.974361	30.333453
433.726676	27487.968401	30.338471
433.853853	27544.369531	30.343488
434.048263	27601.532520	30.348506
434.923412	27649.912319	30.353524
435.181644	27697.182940	30.358541
435.718681	27755.251878	30.363559
436.360014	27809.887740	30.368576
436.921721	27854.244612	30.373594
437.666203	27900.637444	30.378612
437.530301	27941.438220	30.383629
438.303490	27976.632033	30.388647
438.455895	28044.852846	30.393664
439.240323	28075.174790	30.398682
439.620316	28129.492092	30.403700
440.102351	28173.402419	30.408717
440.612637	28211.119424	30.413735
440.783526	28267.326438	30.418752
441.176861	28317.901101	30.423770
441.672144	28362.368037	30.428788
442.203791	28407.217065	30.433805
443.094781	28457.082215	30.438823
443.387769	28493.441506	30.443840
443.726455	28538.578253	30.448858
444.320498	28579.225260	30.453876
444.769867	28619.095045	30.458893
445.822403	28652.834084	30.463911
446.066862	28693.185812	30.468928
446.323591	28729.813405	30.473946
446.680758	28770.301262	30.478964
446.913083	28822.963833	30.483981
447.310616	28864.164450	30.488999
447.540960	28894.569900	30.494016
448.015900	28937.915542	30.499034
448.495544	29001.796027	30.504052
448.643697	29046.101250	30.509069
449.260607	29085.225216	30.514087
449.380623	29144.664199	30.519104
450.013880	29188.921200	30.524122
450.396824	29236.090257	30.529140
450.759456	29289.256367	30.534157
451.704403	29323.793655	30.539175
451.416435	29370.991885	30.544192
451.820491	29406.643906	30.549210
452.506467	29467.444745	30.554228
452.278037	29526.276983	30.559245
453.261998	29572.700994	30.564263
453.642907	29631.761010	30.569280
454.382300	29681.828234	30.574298
455.011047	29729.910714	30.579316
455.084302	29771.633932	30.584333
455.974593	29813.077177	30.589351
456.146032	29874.235730	30.594368
457.090337	29924.982750	30.599386
457.748625	29973.250302	30.604404
458.119424	30015.988068	30.609421
458.507983	30059.637854	30.614439
458.305602	30105.211910	30.619456
458.720135	30154.595967	30.624474
459.730337	30207.370843	30.629492
459.478918	30257.212210	30.634509
460.456916	30306.664513	30.639527
461.070982	30374.789834	30.644544
461.269777	30422.330082	30.649562
461.747485	30470.180871	30.654580
461.829157	30529.697166	30.659597
462.556846	30572.774843	30.664615
463.007036	30634.025670	30.669632
463.259118	30693.088482	30.674650
464.160900	30748.690648	30.679668
464.739141	30808.920874	30.684685
465.361427	30854.865430	30.689703
465.407500	30900.368971	30.694720
466.324962	30959.414264	30.699738
466.791195	31013.802057	30.704756
467.113537	31069.393695	30.709773
467.774081	31114.947726	30.714791
468.195431	31167.153951	30.719808
468.615919	31218.429791	30.724826
469.238682	31259.037310	30.729844
469.597766	31310.134269	30.734861
470.252890	31359.759624	30.739879
470.704552	31413.857664	30.744896
471.564732	31453.088743	30.749914
471.763642	31506.074124	30.754932
471.998973	31560.959220	30.759949
472.868121	31596.526277	30.764967
473.328975	31640.707566	30.769984
473.735295	31691.084819	30.775002
474.032050	31717.669898	30.780020
474.688253	31771.924554	30.785037
474.822259	31825.394864	30.790055
475.317110	31868.283884	30.795072
475.911819	31915.141259	30.800090
476.438901	31967.723623	30.805108
476.750174	32016.133018	30.810125
477.116963	32056.541734	30.815143
477.886993	32118.404321	30.820160
477.945294	32176.731162	30.825178
478.979661	32214.666854	30.830196
479.074877	32277.666854	30.835213
479.338017	32315.222192	30.840231
479.865623	32369.588279	30.845248
480.542464	32431.148698	30.850266
480.994443	32476.658689	30.855284
480.686301	32535.643559	30.860301
481.284021	32587.244339	30.865319
481.885856	32654.522360	30.870336
482.373945	32699.055185	30.875354
482.715265	32749.130695	30.880372
483.225001	32813.960378	30.885389
483.543326	32863.380585	30.890407
484.308986	32928.234673	30.895424
484.772440	32990.277173	30.900442
485.425485	33035.152756	30.905460
486.284258	33075.198580	30.910477
486.953750	33118.831670	30.915495
487.633459	33162.021451	30.920512
487.896686	33208.583643	30.925530
488.598217	33257.894330	30.930548
488.829946	33307.566727	30.935565
489.232459	33346.505319	30.940583
489.508066	33402.938729	30.945600
489.928712	33463.339766	30.950618
490.196445	33523.390790	30.955636
490.187839	33590.511324	30.960653
491.291551	33633.682708	30.965671
491.453913	33697.149976	30.970688
491.617115	33783.812062	30.975706
492.508723	33826.611918	30.980724
492.443618	33900.817201	30.985741
492.845717	33960.547755	30.990759
493.964370	34022.211137	30.995776
494.314365	34093.246940	31.000794
495.359445	34158.611582	31.005812
495.961908	34216.066423	31.010829
496.248869	34282.184668	31.015847
497.063691	34324.461993	31.020864
498.128371	34363.836180	31.025882
498.748644	34414.312087	31.030900
499.048857	34477.311305	31.035917
499.298841	34515.823280	31.040935
499.715844	34573.950471	31.045952
500.034389	34634.126236	31.050970
500.658287	34678.641615	31.055988
501.303843	34750.959687	31.061005
501.477558	34808.439932	31.066023
502.453670	34865.623740	31.071040
502.802681	34927.306955	31.076058
503.313005	34968.638967	31.081076
503.281363	35016.930197	31.086093
503.869177	35080.953775	31.091111
504.836593	35127.827534	31.096128
504.846105	35189.252177	31.101146
505.335636	35259.379721	31.106164
505.765952	35319.911701	31.111181
506.055955	35375.692639	31.116199
506.619260	35446.001223	31.121216
506.651587	35516.359921	31.126234
507.532667	35578.919971	31.131252
507.927438	35650.775061	31.136269
508.814859	35711.254956	31.141287
509.095161	35783.662794	31.146304
510.066705	35843.043689	31.151322
510.882285	35886.681549	31.156340
511.171264	35957.624418	31.161357
511.695565	36024.842823	31.166375
512.080253	36068.489186	31.171392
512.496082	36136.767317	31.176410
512.876791	36202.760437	31.181428
513.631947	36267.117228	31.186445
514.167879	36323.923993	31.191463
514.621042	36386.825795	31.196480
514.869957	36441.711135	31.201498
515.755726	36504.434598	31.206516
516.297789	36565.078568	31.211533
516.726559	36603.849539	31.216551
517.041101	36655.272230	31.221568
517.518174	36731.062845	31.226586
518.143570	36779.815201	31.231604
518.556041	36832.733876	31.236621
518.735932	36902.802239	31.241639
519.534550	36955.253543	31.246656
519.742374	37011.472881	31.251674
520.684847	37078.373695	31.256692
521.017007	37137.984421	31.261709
521.520735	37197.399742	31.266727
522.363867	37261.761352	31.271744
522.519426	37323.759345	31.276762
523.218725	37388.047329	31.281780
523.689042	37454.431055	31.286797
524.264801	37512.528950	31.291815
525.035022	37567.262191	31.296832
525.091044	37635.482366	31.301850
525.661411	37695.999237	31.306868
525.732104	37762.304928	31.311885
526.612833	37832.759801	31.316903
527.409788	37901.388814	31.321920
527.739720	37982.473284	31.326938
528.202461	38044.681814	31.331956
528.642742	38117.249370	31.336973
529.019720	38191.358379	31.341991
530.568682	38244.137671	31.347008
531.358351	38300.482696	31.352026
532.002435	38363.713358	31.357044
532.576199	38414.164041	31.362061
532.907805	38467.296554	31.367079
533.403286	38525.032231	31.372096
533.875945	38596.712641	31.377114
534.284993	38649.444689	31.382132
534.964410	38713.226224	31.387149
535.195938	38773.395524	31.392167
535.985183	38838.898426	31.397184
536.220444	38911.329439	31.402202
536.837790	38961.196860	31.407220
537.448856	39018.021805	31.412237
537.488494	39084.684655	31.417255
538.346516	39138.776907	31.422272
538.809281	39212.995865	31.427290
539.449187	39281.324647	31.432308
540.014197	39347.002142	31.437325
540.264695	39418.113327	31.442343
541.090734	39491.092960	31.447360
541.424642	39558.684246	31.452378
542.399040	39618.686302	31.457396
542.842915	39670.995773	31.462413
542.841698	39733.656025	31.467431
543.397287	39803.708290	31.472448
544.031836	39882.743488	31.477466
544.505944	39953.081235	31.482484
545.156164	40029.655646	31.487501
545.394664	40097.684494	31.492519
546.190090	40182.375988	31.497536
546.476941	40260.333934	31.502554
547.255709	40319.082780	31.507572
547.574747	40380.590751	31.512589
547.868408	40470.151674	31.517607
548.817292	40544.876562	31.522624
549.339762	40624.350145	31.527642
549.958292	40692.820326	31.532660
550.508557	40771.778601	31.537677
550.956864	40852.764783	31.542695
551.524573	40929.776420	31.547712
552.150963	40991.791239	31.552730
552.755334	41042.856537	31.557748
553.330239	41110.094947	31.562765
553.412485	41182.923264	31.567783
554.556810	41243.303492	31.572800
554.887901	41312.811492	31.577818
555.500682	41377.547729	31.582836
556.048655	41453.292698	31.587853
556.438733	41524.780454	31.592871
557.231646	41584.411742	31.597888
557.686607	41658.067411	31.602906
558.222011	41727.590587	31.607924
558.632586	41787.071026	31.612941
559.182303	41865.630043	31.617959
559.728310	41934.454613	31.622976
560.113814	42018.167954	31.627994
560.621797	42099.014040	31.633012
561.575898	42169.473585	31.638029
562.035687	42252.313920	31.643047
562.754773	42319.375104	31.648064
563.105992	42403.212660	31.653082
563.727109	42474.088247	31.658100
564.742616	42540.173168	31.663117
565.284006	42616.984717	31.668135
565.814329	42682.408422	31.673152
566.335196	42760.401470	31.678170
566.731536	42828.363858	31.683188
567.504035	42914.047233	31.688205
567.780967	42986.942079	31.693223
568.643910	43047.112688	31.698240
569.131957	43123.651031	31.703258
569.851945	43200.435509	31.708276
570.169713	43267.304395	31.713293
570.686762	43349.666651	31.718311
571.408904	43419.200089	31.723328
571.931594	43504.062441	31.728346
572.769110	43569.514316	31.733364
573.172040	43644.638741	31.738381
574.032211	43726.974416	31.743399
575.071371	43783.563482	31.748416
575.491376	43852.826431	31.753434
576.254398	43924.615477	31.758452
576.780674	43982.309598	31.763469
576.869060	44060.584765	31.768487
577.769323	44139.168165	31.773504
578.302675	44194.468681	31.778522
578.740527	44266.786326	31.783540
579.370759	44336.590956	31.788557
579.786960	44403.794967	31.793575
579.956425	44479.071827	31.798592
581.141439	44560.179919	31.803610
581.581460	44619.623561	31.808628
582.492950	44702.040328	31.813645
582.665216	44768.436654	31.818663
583.025745	44843.203529	31.823680
583.513975	44929.937696	31.828698
584.111802	45007.428633	31.833716
584.882781	45077.948439	31.838733
585.296096	45151.950087	31.843751
585.907322	45226.910733	31.848768
586.525030	45319.415818	31.853786
587.072301	45389.837986	31.858804
587.826251	45466.020007	31.863821
587.969062	45550.335590	31.868839
588.832673	45615.105209	31.873856
589.521337	45697.250595	31.878874
589.998406	45783.005460	31.883892
590.514270	45849.187847	31.888909
590.729425	45922.306465	31.893927
591.388109	45998.203275	31.898944
591.735851	46073.656028	31.903962
592.161049	46155.925875	31.908980
593.138026	46233.147719	31.913997
593.805876	46318.055736	31.919015
594.476401	46393.955349	31.924032
595.089595	46487.594175	31.929050
595.181934	46556.542367	31.934068
596.608128	46636.937616	31.939085
597.000529	46706.673548	31.944103
597.639043	46773.647272	31.949120
598.179567	46855.313826	31.954138
598.530004	46948.152111	31.959156
599.444502	47013.363376	31.964173
599.851261	47100.882024	31.969191
600.492972	47179.353551	31.974208
601.194970	47261.380428	31.979226
601.605737	47342.353739	31.984244
602.185796	47427.672812	31.989261
602.410914	47522.530269	31.994279
603.251748	47602.732660	31.999296
603.898414	47699.482315	32.004314
604.241125	47796.686857	32.009332
604.912670	47873.192230	32.014349
605.208471	47963.221502	32.019367
605.806775	48056.286389	32.024384
606.703859	48151.149695	32.029402
607.181009	48237.670433	32.034420
608.092291	48332.958610	32.039437
608.799362	48423.837914	32.044455
609.575467	48509.666319	32.049472
610.533699	48600.255517	32.054490
611.107740	48680.503380	32.059508
611.758593	48767.601001	32.064525
612.306474	48849.243372	32.069543
612.853422	48922.539860	32.074560
613.601432	49009.518333	32.079578
614.267765	49094.944350	32.084596
615.241866	49174.177682	32.089613
615.496573	49248.404763	32.094631
616.231272	49338.927030	32.099648
617.170316	49411.920639	32.104666
617.251336	49484.923600	32.109684
618.258724	49565.444692	32.114701
618.870809	49651.952738	32.119719
619.534776	49729.316353	32.124736
620.510165	49801.367510	32.129754
621.055486	49886.295980	32.134772
621.803814	49958.931580	32.139789
622.282008	50033.702737	32.144807
622.542348	50096.853558	32.149824
623.001694	50179.220507	32.154842
623.620927	50263.089944	32.159860
624.499533	50347.059030	32.164877
625.057192	50435.724001	32.169895
625.815333	50495.601012	32.174912
626.606029	50563.936788	32.179930
627.008709	50653.913749	32.184948
627.804202	50729.235278	32.189965
628.020002	50802.909498	32.194983
628.507399	50888.736285	32.200000
629.845983	50977.653778	32.205018
629.875897	51056.880311	32.210036
630.494716	51142.222260	32.215053
631.027531	51224.549982	32.220071
631.496458	51304.444071	32.225088
632.107123	51384.384568	32.230106
632.503681	51480.619898	32.235124
633.151387	51553.742436	32.240141
633.438721	51648.692244	32.245159
634.087952	51739.037833	32.250176
634.305847	51810.672089	32.255194
635.410276	51915.598295	32.260212
635.958791	51994.973598	32.265229
636.784884	52092.830802	32.270247
637.794648	52168.665832	32.275264
638.676988	52256.385413	32.280282
638.770445	52352.027660	32.285300
639.630803	52426.002760	32.290317
640.014157	52514.586071	32.295335
640.368766	52605.107552	32.300352
641.280969	52701.544913	32.305370
641.908010	52797.871923	32.310388
642.753568	52891.737538	32.315405
643.099349	52981.718961	32.320423
643.591176	53075.637569	32.325440
644.605234	53173.848228	32.330458
644.976211	53279.285156	32.335476
645.644342	53371.325116	32.340493
646.205240	53470.572347	32.345511
646.485584	53576.316450	32.350528
647.532130	53672.875434	32.355546
647.942663	53777.297744	32.360564
648.529399	53876.631221	32.365581
649.116058	53984.247460	32.370599
649.566283	54088.885995	32.375616
650.705365	54189.020616	32.380634
650.838421	54310.643807	32.385652
651.814466	54424.585267	32.390669
652.366141	54514.792473	32.395687
653.083652	54624.431237	32.400704
654.157916	54737.492775	32.405722
654.947982	54842.546734	32.410740
655.592393	54941.459128	32.415757
656.112748	55046.167017	32.420775
656.667320	55153.782356	32.425792
657.291866	55251.909863	32.430810
657.790994	55362.056347	32.435828
658.401131	55467.295000	32.440845
659.684155	55575.638957	32.445863
660.176038	55676.924232	32.450880
661.088099	55777.603600	32.455898
661.452923	55877.704139	32.460916
662.297720	55974.333078	32.465933
663.034746	56067.284159	32.470951
663.958801	56172.070376	32.475968
665.130638	56269.487074	32.480986
665.388557	56364.445744	32.486004
665.997512	56452.952781	32.491021
666.645433	56542.780628	32.496039
667.462562	56650.796756	32.501056
668.140436	56741.037570	32.506074
668.504149	56836.606557	32.511092
669.305223	56930.701080	32.516109
669.684385	57040.169087	32.521127
670.527989	57141.877682	32.526144
671.710444	57225.845234	32.531162
672.275862	57325.604055	32.536180
672.974706	57415.484323	32.541197
673.681564	57505.395267	32.546215
674.353776	57602.976876	32.551232
674.966636	57685.144844	32.556250
675.398687	57788.308515	32.561268
676.205301	57883.032199	32.566285
676.875598	57974.726876	32.571303
677.344850	58068.445602	32.576320
677.926862	58146.298506	32.581338
678.701367	58243.101785	32.586356
679.147660	58332.389703	32.591373
679.651435	58422.483668	32.596391
679.755423	58526.406742	32.601408
681.040292	58625.503521	32.606426
681.733639	58723.295659	32.611444
681.986505	58819.555982	32.616461
682.838686	58929.670322	32.621479
683.311390	59034.678901	32.626496
684.060257	59124.419602	32.631514
684.254486	59245.968249	32.636532
685.249801	59367.549636	32.641549
685.985894	59469.774458	32.646567
686.561176	59576.449859	32.651584
687.519073	59687.663104	32.656602
687.823579	59805.929844	32.661620
688.718418	59916.307977	32.666637
689.430900	60029.036061	32.671655
690.003142	60143.380443	32.676672
691.128861	60250.455120	32.681690
691.425486	60361.301019	32.686708
692.349883	60474.483208	32.691725
693.313460	60597.322238	32.696743
693.791713	60704.866475	32.701760
694.823767	60807.548476	32.706778
695.592206	60919.122123	32.711796
696.270403	61019.158804	32.716813
696.822967	61125.410103	32.721831
697.230558	61245.083892	32.726848
697.993250	61358.177665	32.731866
698.866011	61477.763371	32.736884
699.347559	61590.430880	32.741901
700.179996	61709.316781	32.746919
700.522886	61822.153835	32.751936
701.426392	61936.491580	32.756954
702.319121	62053.075371	32.761972
703.246400	62166.797442	32.766989
704.134707	62285.614292	32.772007
704.502040	62390.095249	32.777024
705.494931	62496.502221	32.782042
705.898744	62620.659443	32.787060
706.624572	62729.627191	32.792077
707.477339	62851.240451	32.797095
708.176517	62970.655040	32.802112
709.051780	63083.657663	32.807130
709.485290	63191.020210	32.812148
710.188332	63303.793355	32.817165
710.900813	63418.284736	32.822183
711.395694	63542.843357	32.827200
712.567073	63658.486480	32.832218
713.329922	63773.546700	32.837236
713.835377	63901.955000	32.842253
714.725839	63995.985625	32.847271
715.255352	64114.853408	32.852288
716.133841	64223.032777	32.857306
717.498491	64325.506952	32.862324
718.423438	64419.047122	32.867341
719.193756	64520.274090	32.872359
719.449169	64638.412706	32.877376
720.399251	64731.520329	32.882394
721.423692	64836.726972	32.887412
721.615525	64948.070234	32.892429
722.734406	65039.438396	32.897447
723.045690	65151.888166	32.902464
723.903012	65257.775621	32.907482
724.464769	65369.161201	32.912500
725.310737	65449.343687	32.917517
725.701501	65544.677561	32.922535
726.341691	65660.552409	32.927552
727.488009	65736.027705	32.932570
728.345261	65839.016722	32.937588
728.665524	65941.405913	32.942605
729.633615	66031.659219	32.947623
730.209962	66147.718009	32.952640
730.720918	66238.256309	32.957658
731.324814	66337.566369	32.962676
731.689649	66458.756857	32.967693
732.671503	66566.305614	32.972711
732.602087	66684.642300	32.977728
733.688709	66800.506683	32.982746
735.396894	66896.830301	32.987764
736.436293	66999.548456	32.992781
737.338374	67103.244357	32.997799
737.694466	67216.405935	33.002816
738.124514	67321.299801	33.007834
738.948948	67425.256672	33.012852
739.742124	67535.578892	33.017869
740.449569	67640.302117	33.022887
740.795449	67742.841334	33.027904
741.194083	67866.038429	33.032922
742.215819	67985.649996	33.037940
742.597606	68112.916291	33.042957
743.013182	68231.112098	33.047975
743.912263	68376.413285	33.052992
744.720766	68484.057445	33.058010
745.522653	68617.908199	33.063028
746.008387	68771.410556	33.068045
746.990180	68881.436859	33.073063
747.408053	69016.997326	33.078080
748.687913	69141.048957	33.083098
749.211053	69270.891028	33.088116
750.351752	69400.789973	33.093133
750.837533	69517.887654	33.098151
751.593543	69665.560627	33.103168
752.668867	69789.302117	33.108186
753.651251	69915.639240	33.113204
754.412573	70039.427723	33.118221
755.369676	70148.984204	33.123239
755.926236	70272.276768	33.128256
756.732824	70382.921504	33.133274
757.874308	70497.943677	33.138292
758.379563	70622.738890	33.143309
759.205287	70742.853698	33.148327
760.150778	70859.478224	33.153344
760.834093	70968.875499	33.158362
762.207439	71096.425970	33.163380
762.360373	71217.470199	33.168397
763.141637	71330.014576	33.173415
763.805433	71448.503512	33.178432
764.441897	71571.885256	33.183450
764.891916	71688.779506	33.188468
765.479100	71831.089254	33.193485
766.321182	71958.359550	33.198503
766.445668	72089.517669	33.203520
767.419058	72222.572458	33.208538
768.078681	72360.871218	33.213556
768.344362	72507.500372	33.218573
769.434375	72638.647841	33.223591
770.341824	72797.313664	33.228608
770.747902	72929.391554	33.233626
771.762406	73060.111429	33.238644
772.163100	73222.462074	33.243661
773.289939	73365.780508	33.248679
773.826404	73513.864141	33.253696
774.790913	73640.586683	33.258714
775.216332	73786.635367	33.263732
776.041208	73928.850185	33.268749
776.933462	74058.375833	33.273767
777.810278	74192.078459	33.278784
778.033643	74329.001103	33.283802
779.482117	74464.881243	33.288820
780.127750	74610.045401	33.293837
780.445737	74754.524739	33.298855
781.203032	74893.923948	33.303872
782.481756	75042.407692	33.308890
783.368629	75184.633151	33.313908
784.141044	75321.174149	33.318925
784.978391	75455.144027	33.323943
785.804297	75603.092932	33.328960
786.773016	75758.323673	33.333978
787.525888	75890.697509	33.338996
787.943444	76029.337929	33.344013
788.737641	76169.681509	33.349031
789.829672	76321.714769	33.354048
790.465849	76467.341871	33.359066
791.063675	76613.241898	33.364084
791.911215	76775.570560	33.369101
793.120667	76930.618067	33.374119
793.501042	77069.543150	33.379136
794.547472	77221.027281	33.384154
795.416486	77361.745598	33.389172
795.995152	77515.079888	33.394189
796.821983	77661.404423	33.399207
798.031502	77798.786773	33.404224
798.513406	77956.466239	33.409242
799.738197	78096.687756	33.414260
801.027022	78236.520095	33.419277
802.161880	78370.591438	33.424295
802.981466	78516.891203	33.429312
803.846131	78638.479035	33.434330
804.976310	78764.609338	33.439348
805.821085	78896.802627	33.444365
806.472599	79020.103888	33.449383
807.221809	79154.338523	33.454400
807.768130	79290.897184	33.459418
808.598049	79409.092018	33.464436
809.557168	79532.471826	33.469453
810.559266	79660.285572	33.474471
811.670975	79781.307529	33.479488
812.704645	79917.068462	33.484506
813.495099	80029.080569	33.489524
814.479958	80151.966170	33.494541
814.811868	80283.177039	33.499559
815.789524	80406.413125	33.504576
816.252436	80533.194952	33.509594
817.044181	80655.779950	33.514612
817.566912	80801.700919	33.519629
818.412013	80925.499421	33.524647
819.350428	81061.276686	33.529664
819.902803	81205.563354	33.534682
820.249203	81343.685709	33.539700
820.866474	81473.781024	33.544717
821.851920	81634.793927	33.549735
822.635382	81779.590130	33.554752
823.153120	81923.494900	33.559770
824.136554	82067.709573	33.564788
824.858868	82218.958516	33.569805
825.782962	82365.601419	33.574823
826.723350	82513.045992	33.579840
827.680577	82656.939785	33.584858
828.412176	82796.392818	33.589876
829.045750	82950.077883	33.594893
829.887553	83085.547959	33.599911
831.031301	83233.729104	33.604928
831.587791	83375.378190	33.609946
832.377391	83502.464329	33.614964
833.074871	83644.768727	33.619981
833.610890	83798.058072	33.624999
834.646825	83949.374277	33.630016
835.216283	84099.604427	33.635034
836.007264	84234.564609	33.640052
836.675509	84388.500362	33.645069
837.227055	84554.825020	33.650087
838.222720	84709.341525	33.655104
838.878105	84872.038789	33.660122
839.971346	85019.284494	33.665140
840.828099	85199.033135	33.670157
841.344749	85366.489269	33.675175
842.340641	85504.839584	33.680192
842.961102	85697.405166	33.685210
844.027482	85858.149758	33.690228
845.050215	86020.288300	33.695245
845.923121	86190.836124	33.700263
847.183614	86352.248076	33.705280
848.257661	86505.270450	33.710298
849.182848	86662.507037	33.715316
849.884950	86828.070253	33.720333
850.858823	86985.123819	33.725351
852.390321	87134.442920	33.730368
853.198789	87284.084842	33.735386
854.255906	87431.408788	33.740404
855.180098	87574.263104	33.745421
855.701964	87732.541610	33.750439
856.474795	87877.302043	33.755456
857.204712	88035.478641	33.760474
857.826554	88197.926328	33.765492
858.595913	88353.175184	33.770509
859.126843	88517.937047	33.775527
859.959107	88692.812719	33.780544
860.667859	88853.592710	33.785562
861.499473	89021.693835	33.790580
862.225809	89201.286050	33.795597
863.138950	89368.819331	33.800615
864.419052	89541.380926	33.805632
864.819505	89709.836574	33.810650
865.932419	89887.281913	33.815668
866.538325	90061.034393	33.820685
867.396556	90236.708222	33.825703
868.498924	90419.342072	33.830720
869.153304	90602.861316	33.835738
870.340327	90770.422562	33.840756
871.195261	90950.164994	33.845773
872.150152	91133.075477	33.850791
873.053045	91296.757381	33.855808
873.650146	91474.603493	33.860826
874.570274	91645.208338	33.865844
875.299144	91841.426233	33.870861
876.022032	92015.857126	33.875879
877.125758	92191.245326	33.880896
877.804533	92374.818437	33.885914
879.161655	92543.819629	33.890932
880.594133	92720.176343	33.895949
881.291921	92883.864964	33.900967
882.345544	93044.331476	33.905984
882.888994	93226.180300	33.911002
884.031427	93393.741915	33.916020
884.299913	93568.265397	33.921037
885.139033	93742.202245	33.926055
886.447593	93907.132386	33.931072
887.228998	94084.530609	33.936090
888.607098	94253.382057	33.941108
889.258796	94423.879975	33.946125
890.121231	94573.197986	33.951143
891.214369	94725.915668	33.956160
892.033623	94890.977575	33.961178
892.769706	95050.921142	33.966196
893.441110	95227.263506	33.971213
894.051274	95395.477456	33.976231
895.084604	95558.938797	33.981248
895.626515	95739.914169	33.986266
896.549155	95915.428796	33.991284
897.262295	96091.333731	33.996301
898.004277	96268.513774	34.001319
898.899150	96434.580015	34.006336
899.916740	96641.182520	34.011354
900.828529	96825.326697	34.016372
901.562996	97014.084413	34.021389
902.270035	97202.879748	34.026407
903.848475	97379.689111	34.031424
904.551115	97572.843066	34.036442
905.953155	97743.430008	34.041460
906.676655	97931.690106	34.046477
907.804437	98113.560966	34.051495
908.715159	98288.815863	34.056512
909.263629	98484.553451	34.061530
910.400099	98662.590698	34.066548
911.143307	98853.576560	34.071565
911.823718	99051.847964	34.076583
912.824920	99231.475219	34.081600
913.120255	99438.302488	34.086618
914.070784	99633.229324	34.091636
915.214446	99835.785898	34.096653
915.732464	100044.113400	34.101671
916.714993	100242.616529	34.106688
917.443611	100448.867757	34.111706
917.965313	100663.492600	34.116724
919.518645	100865.616272	34.121741
920.729987	101079.864878	34.126759
921.608279	101291.720168	34.131776
922.015674	101505.744232	34.136794
922.968673	101710.252938	34.141812
924.410748	101920.032394	34.146829
925.964182	102098.854407	34.151847
927.474279	102291.487029	34.156864
928.325644	102504.116591	34.161882
929.587742	102678.058644	34.166900
930.807004	102860.391759	34.171917
931.563655	103046.335509	34.176935
932.709251	103230.861443	34.181952
933.385443	103430.484673	34.186970
934.346031	103611.985736	34.191988
935.285328	103801.862042	34.197005
936.018239	103984.283413	34.202023
936.454909	104182.571690	34.207040
937.529257	104380.414283	34.212058
938.560797	104555.648104	34.217076
940.455614	104726.865465	34.222093
941.139212	104919.014665	34.227111
942.349800	105080.640479	34.232128
943.866084	105254.291969	34.237146
944.890489	105431.584443	34.242164
945.615487	105599.530722	34.247181
946.024674	105780.333804	34.252199
947.211927	105945.381850	34.257216
947.860242	106130.099145	34.262234
948.461718	106318.992106	34.267252
949.693098	106496.840189	34.272269
950.199821	106683.205822	34.277287
951.078621	106858.011704	34.282304
951.351816	107044.975701	34.287322
952.164887	107222.353157	34.292340
953.062896	107410.014473	34.297357
953.650313	107599.235552	34.302375
954.550553	107794.599640	34.307392
955.503685	107994.034673	34.312410
956.539729	108197.447128	34.317428
957.280048	108389.751630	34.322445
957.844704	108601.300276	34.327463
959.187964	108798.536437	34.332480
960.136424	109007.023156	34.337498
961.361728	109207.625591	34.342516
962.484823	109407.043133	34.347533
963.420081	109628.671530	34.352551
964.705502	109820.592339	34.357568
965.623196	110032.283996	34.362586
966.497673	110225.098848	34.367604
967.490353	110423.684150	34.372621
968.216975	110640.681389	34.377639
969.118341	110834.484149	34.382656
970.249631	111064.806666	34.387674
971.139860	111277.348620	34.392692
972.179550	111478.061933	34.397709
972.547790	111698.344218	34.402727
973.798723	111911.768944	34.407744
974.705442	112130.559762	34.412762
975.917769	112350.454609	34.417780
976.758989	112565.446840	34.422797
977.943246	112782.423604	34.427815
979.716002	112996.100001	34.432832
980.365741	113216.601389	34.437850
981.380101	113442.884242	34.442868
982.385687	113645.417922	34.447885
983.220871	113866.729982	34.452903
984.276425	114076.669407	34.457920
985.355276	114300.972408	34.462938
985.920547	114525.095979	34.467956
987.364615	114732.898617	34.472973
988.315355	114950.260353	34.477991
989.326666	115166.574953	34.483008
990.515534	115378.491190	34.488026
991.424812	115591.088639	34.493044
992.462902	115810.659708	34.498061
992.865797	116026.422623	34.503079
993.922963	116256.091279	34.508096
994.993050	116482.719053	34.513114
995.904883	116712.187381	34.518132
996.791240	116925.799599	34.523149
997.521018	117173.317727	34.528167
998.805510	117394.228784	34.533184
999.592625	117623.154963	34.538202
1000.553273	117858.123215	34.543220
1001.542544	118094.013594	34.548237
1002.807996	118323.373242	34.553255
1003.900513	118560.162682	34.558272
1004.616322	118794.013415	34.563290
1005.133325	119030.356940	34.568308
1006.706359	119285.077705	34.573325
1007.534852	119512.428390	34.578343
1008.770922	119734.569272	34.583360
1010.038209	119977.132077	34.588378
1010.940523	120209.227634	34.593396
1011.897191	120436.551776	34.598413
1012.908928	120671.902105	34.603431
1014.308148	120905.074279	34.608448
1015.341982	121140.906272	34.613466
1016.494953	121355.242431	34.618484
1017.533723	121567.014031	34.623501
1018.152826	121796.520682	34.628519
1019.209884	122000.980886	34.633536
1020.239087	122222.465343	34.638554
1020.935066	122440.610417	34.643572
1022.183765	122660.401924	34.648589
1023.087596	122894.013897	34.653607
1024.103693	123130.587153	34.658624
1024.985903	123351.407406	34.663642
1025.426016	123587.572517	34.668660
1026.540085	123810.436189	34.673677
1027.706733	124064.125255	34.678695
1028.258686	124289.949330	34.683712
1029.357040	124538.343859	34.688730
1030.623245	124794.227776	34.693748
1031.614597	125026.739544	34.698765
1032.136333	125280.482057	34.703783
1033.208840	125534.630044	34.708800
1034.890602	125784.674830	34.713818
1035.878811	126042.376881	34.718836
1036.954900	126284.161341	34.723853
1037.667978	126542.572105	34.728871
1038.736744	126789.456615	34.733888
1039.727756	127056.114500	34.738906
1041.033482	127308.832108	34.743924
1041.923372	127556.943734	34.748941
1043.077634	127818.448349	34.753959
1044.091838	128070.878193	34.758976
1045.113763	128332.485093	34.763994
1046.275504	128586.390402	34.769012
1047.468134	128843.499379	34.774029
1048.811241	129109.660745	34.779047
1049.694201	129361.691911	34.784064
1050.751365	129617.232670	34.789082
1051.647664	129880.369076	34.794100
1053.029938	130142.616276	34.799117
1054.146581	130389.927419	34.804135
1055.912036	130654.371861	34.809152
1056.675557	130886.268657	34.814170
1058.034831	131139.705940	34.819188
1059.003400	131403.033385	34.824205
1059.989031	131662.747633	34.829223
1061.128677	131903.298081	34.834240
1062.089400	132145.565799	34.839258
1063.063832	132406.073922	34.844276
1064.112050	132659.359283	34.849293
1065.175643	132901.882001	34.854311
1066.129496	133162.868753	34.859328
1067.862454	133413.942813	34.864346
1068.776916	133660.970712	34.869364
1069.883598	133906.637739	34.874381
1071.695026	134140.084033	34.879399
1072.817933	134382.709614	34.884416
1073.977390	134609.294696	34.889434
1074.957979	134856.511028	34.894452
1075.956429	135096.259491	34.899469
1077.230198	135321.512281	34.904487
1077.941561	135562.160957	34.909504
1079.742412	135793.567238	34.914522
1080.136379	136023.724152	34.919540
1081.390020	136260.992335	34.924557
1082.176305	136518.978609	34.929575
1082.847910	136761.240078	34.934592
1083.915422	137000.293876	34.939610
1084.839636	137257.274314	34.944628
1086.031576	137502.536089	34.949645
1086.937368	137752.296947	34.954663
1087.667262	138009.898517	34.959680
1088.877840	138248.227756	34.964698
1089.738304	138500.803647	34.969716
1090.982287	138746.256214	34.974733
1091.889660	138977.540767	34.979751
1092.595740	139230.173025	34.984768
1093.787525	139494.315424	34.989786
1094.809342	139742.537919	34.994804
1096.212014	139985.691180	34.999821
1097.461074	140237.506001	35.004839
1098.543989	140488.475266	35.009856
1099.688422	140731.169361	35.014874
1100.394494	140995.517814	35.019892
1101.959800	141252.892258	35.024909
1103.138096	141494.330951	35.029927
1103.970368	141762.633224	35.034944
1104.967208	142014.059064	35.039962
1106.335262	142270.966555	35.044980
1107.134435	142540.003127	35.049997
1107.972814	142802.784076	35.055015
1108.907768	143080.031786	35.060032
1110.270643	143353.356289	35.065050
1111.069465	143639.177421	35.070068
1112.456275	143895.535967	35.075085
1114.060499	144174.102145	35.080103
1114.692065	144450.637360	35.085120
1115.772456	144715.193471	35.090138
1116.751573	145003.963302	35.095156
1118.071758	145285.172093	35.100173
1119.108848	145568.255928	35.105191
1120.276359	145852.030645	35.110208
1121.642857	146127.823657	35.115226
1122.701580	146419.356422	35.120244
1123.660621	146697.681293	35.125261
1124.680262	146976.683134	35.130279
1125.831436	147275.410740	35.135296
1126.914680	147555.129440	35.140314
1128.120737	147844.912101	35.145332
1129.362466	148139.269383	35.150349
1130.695426	148420.094948	35.155367
1131.791526	148706.567293	35.160384
1133.445911	148989.195798	35.165402
1134.579165	149270.631605	35.170420
1135.091841	149555.253852	35.175437
1136.685966	149839.725159	35.180455
1137.428911	150132.747762	35.185472
1138.889009	150425.070910	35.190490
1139.301380	150719.750770	35.195508
1140.698234	151017.606079	35.200525
1141.992540	151307.388929	35.205543
1142.858311	151603.763907	35.210560
1144.320022	151896.060331	35.215578
1145.349377	152193.668626	35.220596
1147.202180	152476.202272	35.225613
1149.494508	152741.593468	35.230631
1150.594068	153021.211499	35.235648
1152.158858	153273.155066	35.240666
1153.231126	153552.324914	35.245684
1154.374758	153819.333874	35.250701
1155.447851	154087.726220	35.255719
1155.872624	154375.837029	35.260736
1157.154202	154636.943530	35.265754
1157.850183	154908.727128	35.270772
1159.089380	155183.568691	35.275789
1160.233316	155476.211502	35.280807
1160.856735	155756.143764	35.285824
1161.836484	156030.742429	35.290842
1162.786434	156336.209835	35.295860
1163.990600	156615.215225	35.300877
1165.470164	156909.551235	35.305895
1166.384495	157185.995445	35.310912
1167.453996	157459.257402	35.315930
1168.617534	157748.730052	35.320948
1169.475102	158026.331186	35.325965
1170.849375	158311.891481	35.330983
1171.998317	158605.457475	35.336000
1173.095948	158887.883520	35.341018
1174.218770	159175.762218	35.346036
1175.294484	159461.227787	35.351053
1177.036458	159749.820286	35.356071
1177.715011	160047.698854	35.361088
1179.008071	160336.293528	35.366106
1180.324607	160638.726889	35.371124
1181.686668	160924.967431	35.376141
1182.988418	161209.126705	35.381159
1184.256133	161504.876203	35.386176
1185.788474	161792.984977	35.391194
1186.706840	162091.079915	35.396212
1187.839495	162400.293173	35.401229
1189.214106	162665.864580	35.406247
1190.153134	162984.654555	35.411264
1191.134498	163273.765339	35.416282
1192.506892	163569.410806	35.421300
1193.762256	163873.971310	35.426317
1194.891288	164179.531783	35.431335
1195.689169	164495.869860	35.436352
1197.133411	164785.371370	35.441370
1198.115231	165101.099983	35.446388
1199.149283	165411.112924	35.451405
1200.932542	165712.541807	35.456423
1202.191905	166016.305009	35.461440
1203.369851	166330.513166	35.466458
1204.507192	166634.453121	35.471476
1205.776395	166951.391312	35.476493
1207.217228	167260.677954	35.481511
1208.188293	167572.417016	35.486528
1209.318933	167877.013851	35.491546
1210.755737	168192.943707	35.496564
1211.700603	168511.888056	35.501581
1213.244615	168814.748275	35.506599
1213.983511	169149.871018	35.511616
1215.847703	169454.915951	35.516634
1217.239058	169756.031358	35.521652
1218.173484	170067.730598	35.526669
1219.875406	170394.925435	35.531687
1220.520822	170696.868161	35.536704
1221.834943	171010.084683	35.541722
1223.177732	171330.734521	35.546740
1223.693519	171654.873098	35.551757
1225.154354	171961.778040	35.556775
1226.179476	172294.326281	35.561792
1227.306185	172619.817432	35.566810
1228.496911	172953.244044	35.571828
1228.933408	173276.011239	35.576845
1230.855574	173618.928046	35.581863
1231.903670	173955.380175	35.586880
1233.377561	174290.279698	35.591898
1235.092006	174612.286797	35.596916
1236.403254	174946.304127	35.601933
1237.978642	175263.909719	35.606951
1239.444299	175583.426406	35.611968
1240.747717	175890.928749	35.616986
1242.088160	176200.076721	35.622004
1243.242614	176522.544464	35.627021
1245.006108	176827.781366	35.632039
1245.947534	177147.103054	35.637056
1247.121563	177456.311884	35.642074
1248.583452	177750.030264	35.647092
1249.423891	178046.606926	35.652109
1250.616722	178345.855796	35.657127
1251.966845	178646.311558	35.662144
1252.961762	178936.890512	35.667162
1254.110419	179253.018819	35.672180
1254.731896	179562.712749	35.677197
1256.379202	179867.086526	35.682215
1257.218685	180190.582062	35.687232
1258.482204	180514.326969	35.692250
1259.833229	180815.988574	35.697268
1261.248092	181140.105923	35.702285
1262.272430	181471.067249	35.707303
1263.667685	181783.591511	35.712320
1265.060909	182101.867497	35.717338
1266.534877	182430.247732	35.722356
1268.058514	182746.234250	35.727373
1269.402690	183052.390398	35.732391
1270.775481	183382.506772	35.737408
1272.186226	183691.219508	35.742426
1273.362350	184013.198359	35.747444
1274.167169	184344.467953	35.752461
1275.907524	184667.842668	35.757479
1276.796426	184991.194860	35.762496
1277.795334	185327.566359	35.767514
1279.029316	185659.154008	35.772532
1280.345772	185987.747220	35.777549
1281.491464	186330.713741	35.782567
1282.507673	186680.266128	35.787584
1283.791365	187015.077847	35.792602
1285.274747	187356.027571	35.797620
1286.228565	187716.779589	35.802637
1287.949546	188049.811762	35.807655
1288.940775	188415.753727	35.812672
1289.839927	188763.942212	35.817690
1291.552234	189113.521869	35.822708
1292.625333	189477.261166	35.827725
1294.110232	189830.246592	35.832743
1295.605721	190189.312825	35.837760
1296.782360	190542.658142	35.842778
1298.593313	190902.603389	35.847796
1299.525525	191250.839547	35.852813
1300.857733	191607.796159	35.857831
1302.348013	191962.050342	35.862848
1303.122924	192328.522455	35.867866
1304.946159	192684.173147	35.872884
1305.450579	193061.725879	35.877901
1306.760158	193439.922459	35.882919
1308.073513	193811.011746	35.887936
1309.240251	194184.679138	35.892954
1311.204738	194559.131174	35.897972
1312.098528	194940.528592	35.902989
1313.759733	195297.833532	35.908007
1315.158282	195683.988998	35.913024
1316.827493	196038.986349	35.918042
1318.774111	196392.124498	35.923060
1320.005824	196765.517340	35.928077
1321.147596	197114.920270	35.933095
1322.554923	197461.005855	35.938112
1323.869168	197827.167555	35.943130
1325.288952	198178.015735	35.948148
1326.245334	198534.147495	35.953165
1327.474134	198906.156653	35.958183
1328.617985	199280.886130	35.963200
1329.977559	199639.115592	35.968218
1331.036123	200004.354020	35.973236
1332.486120	200378.074235	35.978253
1333.782157	200741.271496	35.983271
1334.942224	201098.272033	35.988288
1335.994043	201456.752360	35.993306
1337.522487	201811.423191	35.998324
1338.331458	202173.349913	36.003341
1339.690758	202540.951851	36.008359
1341.407008	202912.407316	36.013376
1342.640869	203279.944943	36.018394
1343.843108	203647.375420	36.023412
1344.996279	204011.870259	36.028429
1346.697167	204377.038355	36.033447
1347.672148	204752.155404	36.038464
1349.261123	205128.798248	36.043482
1350.617533	205504.287897	36.048500
1351.973532	205878.814551	36.053517
1353.434811	206257.782377	36.058535
1355.158828	206625.573397	36.063552
1356.622948	207000.329059	36.068570
1358.206446	207369.670546	36.073588
1359.615173	207762.113641	36.078605
1360.966105	208124.678695	36.083623
1361.931194	208497.225801	36.088640
1363.004268	208886.720690	36.093658
1365.017421	209243.848706	36.098676
1366.387887	209635.317115	36.103693
1368.412422	210004.560177	36.108711
1369.874780	210368.818628	36.113728
1370.913828	210738.646710	36.118746
1372.532863	211116.558152	36.123764
1373.981426	211490.690098	36.128781
1375.488350	211865.677561	36.133799
1376.786358	212225.450887	36.138816
1377.921819	212602.953664	36.143834
1379.508441	212988.891400	36.148852
1380.520527	213368.170269	36.153869
1381.583007	213749.271033	36.158887
1383.371713	214138.888451	36.163904
1384.331394	214522.549213	36.168922
1385.438893	214910.961842	36.173940
1386.539414	215308.393214	36.178957
1387.950992	215708.441694	36.183975
1389.385975	216107.472192	36.188992
1390.329947	216522.407939	36.194010
1391.845762	216940.908396	36.199028
1393.143424	217345.808296	36.204045
1394.367472	217750.239533	36.209063
1395.547175	218174.591589	36.214080
1396.919996	218591.776872	36.219098
1398.471067	219008.528169	36.224116
1399.961072	219443.882662	36.229133
1401.338783	219885.378550	36.234151
1403.229063	220337.967025	36.239168
1404.866165	220752.400193	36.244186
1405.963376	221179.521769	36.249204
1407.262897	221603.462304	36.254221
1408.719025	222012.444310	36.259239
1410.731534	222430.682824	36.264256
1411.819396	222854.434728	36.269274
1413.597551	223260.777697	36.274292
1414.836504	223685.676267	36.279309
1416.237133	224097.520035	36.284327
1417.805204	224507.966135	36.289344
1418.995918	224932.623426	36.294362
1420.625556	225338.033303	36.299380
1422.351084	225763.722988	36.304397
1423.383112	226178.962435	36.309415
1425.094107	226600.746013	36.314432
1426.907003	226997.952679	36.319450
1428.388074	227389.144842	36.324468
1429.614827	227798.744377	36.329485
1431.197163	228182.911967	36.334503
1432.696022	228566.510306	36.339520
1433.467821	228962.980671	36.344538
1434.957096	229348.208550	36.349556
1436.009327	229753.474347	36.354573
1437.373259	230160.010773	36.359591
1438.318161	230568.446419	36.364608
1439.339077	231003.465140	36.369626
1440.917697	231420.714359	36.374644
1442.068577	231843.115557	36.379661
1443.265011	232266.983744	36.384679
1444.550434	232712.708646	36.389696
1445.919266	233160.554825	36.394714
1447.155263	233590.364153	36.399732
1448.446207	234050.977168	36.404749
1449.730925	234509.560502	36.409767
1451.248054	234964.322048	36.414784
1452.672573	235440.056270	36.419802
1454.150380	235903.361818	36.424820
1455.598656	236367.206974	36.429837
1457.168887	236833.878261	36.434855
1459.102842	237297.544216	36.439872
1460.595705	237768.422061	36.444890
1462.125387	238239.980924	36.449908
1463.441978	238704.717688	36.454925
1464.854658	239183.918824	36.459943
1466.633356	239642.942445	36.464960
1467.962958	240125.614307	36.469978
1469.637494	240593.751256	36.474996
1471.176367	241066.839681	36.480013
1472.596469	241536.316273	36.485031
1474.090645	242020.032323	36.490048
1475.722882	242490.161848	36.495066
1477.302482	242971.960714	36.500084
1479.071067	243450.147668	36.505101
1480.538353	243920.307336	36.510119
1482.017689	244391.024779	36.515136
1483.225226	244865.852363	36.520154
1484.946715	245350.680836	36.525172
1486.837470	245821.256796	36.530189
1488.204300	246290.522873	36.535207
1489.863700	246775.897570	36.540224
1490.838080	247256.712003	36.545242
1492.101718	247732.779953	36.550260
1493.723294	248219.433342	36.555277
1495.432447	248705.564948	36.560295
1497.045119	249186.759606	36.565312
1498.257163	249667.843206	36.570330
1499.880975	250161.408550	36.575348
1501.271675	250644.928001	36.580365
1502.862923	251132.301600	36.585383
1504.581955	251603.066480	36.590400
1506.315587	252105.481680	36.595418
1507.566644	252580.694110	36.600436
1509.966464	253066.107313	36.605453
1510.776939	253543.832029	36.610471
1512.737536	254010.164569	36.615488
1514.833741	254486.026689	36.620506
1516.261315	254952.701913	36.625524
1517.752514	255434.837508	36.630541
1519.010956	255909.340033	36.635559
1520.300942	256380.840036	36.640576
1521.498665	256866.632133	36.645594
1522.885019	257359.861891	36.650612
1524.693797	257842.251155	36.655629
1525.963088	258326.304606	36.660647
1527.341082	258813.160025	36.665664
1528.502886	259283.234242	36.670682
1529.946971	259753.770025	36.675700
1531.869893	260231.619214	36.680717
1533.257658	260705.924062	36.685735
1534.890061	261163.066715	36.690752
1536.321369	261641.581305	36.695770
1537.575243	262122.817872	36.700788
1538.944579	262606.347009	36.705805
1540.771507	263086.244073	36.710823
1542.316905	263564.942698	36.715840
1543.668991	264064.071890	36.720858
1544.827998	264539.912542	36.725876
1546.732565	265043.319508	36.730893
1547.889844	265542.734187	36.735911
1549.496419	266038.619600	36.740928
1551.025020	266546.787306	36.745946
1552.234880	267053.000387	36.750964
1554.165540	267567.527989	36.755981
1555.159588	268085.080246	36.760999
1557.130169	268589.185061	36.766016
1558.217934	269115.865983	36.771034
1559.957323	269639.669884	36.776052
1561.554267	270161.515255	36.781069
1563.113418	270695.940718	36.786087
1564.795617	271222.190830	36.791104
1566.040685	271759.892871	36.796122
1568.044274	272279.483728	36.801140
1570.787442	272788.739844	36.806157
1572.670686	273303.928924	36.811175
1574.464875	273832.290520	36.816192
1575.657864	274344.467267	36.821210
1577.262719	274855.482867	36.826228
1579.118097	275366.710256	36.831245
1580.484477	275890.540872	36.836263
1582.322620	276392.522649	36.841280
1583.489297	276916.333385	36.846298
1585.442152	277433.053048	36.851316
1586.989555	277946.460001	36.856333
1588.800954	278480.144150	36.861351
1590.484196	278992.967541	36.866368
1591.570477	279505.659633	36.871386
1593.021496	280036.402072	36.876404
1594.557084	280558.136888	36.881421
1595.984691	281094.646774	36.886439
1597.881514	281628.207387	36.891456
1599.357113	282156.349238	36.896474
1600.230430	282686.113108	36.901492
1601.943662	283231.409761	36.906509
1603.229041	283785.437336	36.911527
1604.851732	284328.205430	36.916544
1606.235533	284878.047452	36.921562
1607.980307	285437.734682	36.926580
1610.193492	285981.238293	36.931597
1612.140493	286517.798655	36.936615
1614.064603	287068.458617	36.941632
1615.999188	287610.529338	36.946650
1617.117182	288150.243561	36.951668
1619.694080	288671.045476	36.956685
1620.894225	289213.637958	36.961703
1622.680409	289749.857726	36.966720
1624.194277	290273.699491	36.971738
1625.905848	290808.759074	36.976756
1627.639248	291340.460095	36.981773
1629.000012	291877.554542	36.986791
1630.663959	292410.456537	36.991808
1631.929709	292952.489858	36.996826
1633.156113	293496.406952	37.001844
1634.703630	294031.988339	37.006861
1636.287688	294563.243403	37.011879
1637.976859	295093.005607	37.016896
1639.521203	295614.890094	37.021914
1640.840925	296143.260765	37.026932
1642.361663	296683.889110	37.031949
1643.618313	297216.684712	37.036967
1645.644810	297761.542308	37.041984
1647.170913	298304.473256	37.047002
1648.606412	298859.226880	37.052020
1650.148283	299396.993777	37.057037
1651.319126	299969.742129	37.062055
1653.138579	300529.071566	37.067072
1654.618150	301087.869870	37.072090
1656.370011	301655.992068	37.077108
1657.860713	302232.687833	37.082125
1659.245016	302822.147472	37.087143
1660.636789	303394.814452	37.092160
1662.426755	303994.054286	37.097178
1663.953363	304590.463869	37.102196
1665.851987	305187.443185	37.107213
1667.267702	305785.869733	37.112231
1669.063348	306384.204252	37.117248
1670.764564	306994.207417	37.122266
1672.262334	307604.620879	37.127284
1673.991912	308203.080956	37.132301
1676.010186	308828.917054	37.137319
1677.353157	309421.159544	37.142336
1679.286348	310043.165889	37.147354
1681.386448	310666.638365	37.152372
1683.213190	311268.971447	37.157389
1684.804626	311892.493046	37.162407
1686.241257	312511.184873	37.167424
1688.119785	313120.377482	37.172442
1689.654477	313748.287070	37.177460
1691.603803	314366.625641	37.182477
1693.506755	314996.368818	37.187495
1695.116381	315620.238329	37.192512
1696.673525	316243.298668	37.197530
1698.277339	316874.167234	37.202548
1700.317013	317497.670545	37.207565
1701.754522	318128.276284	37.212583
1703.654181	318760.831617	37.217600
1705.016658	319396.897889	37.222618
1706.507668	320019.606143	37.227636
1708.871866	320667.886961	37.232653
1710.695418	321299.873023	37.237671
1712.410532	321919.403738	37.242688
1714.683154	322550.592961	37.247706
1716.005266	323184.649818	37.252724
1717.993623	323804.904894	37.257741
1719.391572	324449.702669	37.262759
1721.161622	325078.969793	37.267776
1724.662673	325679.584259	37.272794
1726.633153	326296.339595	37.277812
1728.289340	326892.346506	37.282829
1729.929649	327502.974606	37.287847
1731.723476	328104.380390	37.292864
1733.365550	328705.170515	37.297882
1734.798627	329326.985554	37.302900
1736.861343	329920.001305	37.307917
1738.907606	330519.335462	37.312935
1740.237877	331107.433197	37.317952
1742.277528	331716.505082	37.322970
1743.388754	332331.207350	37.327988
1745.490873	332929.542551	37.333005
1746.984592	333543.051565	37.338023
1748.507616	334158.376861	37.343040
1750.274862	334752.102110	37.348058
1751.996098	335346.209344	37.353076
1753.389082	335932.545471	37.358093
1754.923149	336525.299894	37.363111
1756.569004	337112.800004	37.368128
1758.140251	337716.476137	37.373146
1759.710744	338323.140902	37.378164
1761.265743	338921.348251	37.383181
1762.914166	339539.231323	37.388199
1764.429429	340154.133710	37.393216
1766.353889	340777.058537	37.398234
1767.277294	341399.658612	37.403252
1769.404738	342035.251438	37.408269
1771.018376	342678.637233	37.413287
1772.487092	343325.566734	37.418304
1774.173163	343966.461807	37.423322
1775.601065	344630.868916	37.428340
1777.508551	345295.060928	37.433357
1779.217239	345948.439014	37.438375
1780.636174	346611.652810	37.443392
1782.802800	347296.027843	37.448410
1784.663039	347972.956480	37.453428
1786.272332	348658.038081	37.458445
1788.131788	349338.170170	37.463463
1789.740348	350026.733887	37.468480
1792.051576	350708.598373	37.473498
1793.597246	351401.212166	37.478516
1795.982300	352073.654086	37.483533
1797.957174	352756.456594	37.488551
1799.573676	353447.301321	37.493568
1801.554165	354133.659698	37.498586
1803.197859	354820.798738	37.503604
1805.084726	355518.823557	37.508621
1806.795446	356222.220223	37.513639
1808.503676	356913.299057	37.518656
1810.699812	357605.757839	37.523674
1811.997337	358319.286767	37.528692
1813.969817	359018.533885	37.533709
1815.365731	359732.605943	37.538727
1817.455514	360435.463421	37.543744
1819.705673	361145.107417	37.548762
1821.151999	361869.282619	37.553780
1823.029269	362569.981609	37.558797
1825.374941	363287.335669	37.563815
1827.044047	364007.173174	37.568832
1829.266543	364711.329274	37.573850
1830.715548	365433.003604	37.578868
1832.627266	366144.364618	37.583885
1834.667250	366854.118548	37.588903
1836.492232	367569.551845	37.593920
1838.179605	368284.943686	37.598938
1839.999524	369009.584421	37.603956
1842.118515	369717.141034	37.608973
1844.534613	370432.549401	37.613991
1846.529812	371137.258479	37.619008
1848.734158	371830.885855	37.624026
1850.520399	372543.592403	37.629044
1852.137986	373245.355604	37.634061
1854.385324	373945.707788	37.639079
1855.700068	374651.475661	37.644096
1858.116118	375352.026176	37.649114
1860.094330	376039.852670	37.654132
1862.219442	376725.384364	37.659149
1864.551452	377428.570494	37.664167
1865.896321	378120.416993	37.669184
1867.957338	378805.233661	37.674202
1869.597305	379503.140930	37.679220
1871.482638	380187.401135	37.684237
1873.559884	380875.724008	37.689255
1875.063736	381544.322950	37.694272
1876.856881	382208.524791	37.699290
1878.371275	382883.282559	37.704308
1880.218465	383547.322088	37.709325
1882.092441	384230.969340	37.714343
1883.647259	384906.668119	37.719360
1885.396021	385586.352395	37.724378
1887.596494	386274.669864	37.729396
1889.086797	386955.965449	37.734413
1891.004978	387643.970721	37.739431
1892.643146	388348.080999	37.744448
1894.215714	389038.496417	37.749466
1896.484843	389757.378442	37.754484
1898.309910	390455.478835	37.759501
1900.560719	391148.448734	37.764519
1902.115507	391860.758557	37.769536
1904.327263	392571.042469	37.774554
1906.766631	393267.127932	37.779572
1908.943478	393967.119159	37.784589
1910.937167	394667.884965	37.789607
1912.846930	395382.639934	37.794624
1914.446876	396074.186520	37.799642
1916.396744	396794.072029	37.804660
1918.130520	397515.141714	37.809677
1919.812424	398228.168260	37.814695
1921.496878	398962.871544	37.819712
1923.720505	399684.745242	37.824730
1925.609600	400410.989889	37.829748
1927.277351	401151.596473	37.834765
1929.085203	401890.209720	37.839783
1931.133183	402622.657314	37.844800
1933.368150	403367.725340	37.849818
1934.900494	404116.487956	37.854836
1936.991829	404851.354355	37.859853
1939.210453	405598.342850	37.864871
1940.649883	406355.068149	37.869888
1942.848285	407104.224111	37.874906
1944.886611	407847.939023	37.879924
1946.705140	408606.541956	37.884941
1948.557208	409376.848308	37.889959
1950.343205	410141.646402	37.894976
1951.964217	410900.015578	37.899994
1954.209061	411673.561375	37.905012
1956.078683	412448.692049	37.910029
1958.142115	413221.387202	37.915047
1959.750248	414006.622814	37.920064
1961.932091	414774.693811	37.925082
1963.938466	415560.450800	37.930100
1966.052821	416347.660781	37.935117
1968.239577	417125.008120	37.940135
1970.286366	417914.841182	37.945152
1972.376935	418675.771630	37.950170
1974.190615	419472.483954	37.955188
1975.773199	420261.738962	37.960205
1977.941750	421041.022076	37.965223
1979.967508	421838.511638	37.970240
1981.842824	422634.785318	37.975258
1983.858521	423424.933526	37.980276
1985.488758	424219.703208	37.985293
1987.106860	425030.071434	37.990311
1989.185160	425844.033655	37.995328
1991.251370	426628.248027	38.000346
1993.020484	427461.853971	38.005364
1995.159437	428274.104995	38.010381
1997.428593	429070.814462	38.015399
1998.885495	429893.300160	38.020416
2001.034071	430695.089122	38.025434
2003.169571	431500.194539	38.030452
2004.916379	432296.983909	38.035469
2007.316839	433091.006283	38.040487
2009.119326	433873.862844	38.045504
2011.488286	434655.334342	38.050522
2013.740008	435446.618565	38.055540
2015.474773	436237.910432	38.060557
2017.789406	437006.911027	38.065575
2019.388825	437798.728345	38.070592
2021.676945	438583.218120	38.075610
2023.673764	439379.014460	38.080628
2025.590433	440167.002756	38.085645
2027.694017	440959.588312	38.090663
2029.940040	441766.341715	38.095680
2031.681833	442569.404731	38.100698
2033.617256	443376.505358	38.105716
2035.877478	444177.097220	38.110733
2037.793267	444985.862656	38.115751
2039.782084	445804.856705	38.120768
2041.855079	446617.836426	38.125786
2044.110459	447430.199230	38.130804
2045.786361	448252.491725	38.135821
2048.195617	449054.751799	38.140839
2050.204511	449884.059648	38.145856
2052.465803	450708.539037	38.150874
2054.548141	451530.234129	38.155892
2056.600064	452357.111905	38.160909
2058.784137	453172.758238	38.165927
2060.609723	454014.072977	38.170944
2062.648832	454836.455395	38.175962
2064.644311	455686.221373	38.180980
2066.635333	456525.991437	38.185997
2068.860596	457381.616892	38.191015
2070.797930	458222.944744	38.196032
2073.316226	459053.979351	38.201050
2075.745881	459900.314182	38.206068
2078.117382	460736.511845	38.211085
2080.044073	461569.714942	38.216103
2081.850117	462423.781852	38.221120
2083.812690	463254.179261	38.226138
2085.836000	464115.569052	38.231156
2087.903064	464961.295376	38.236173
2090.400278	465808.077121	38.241191
2092.754972	466653.127517	38.246208
2095.086018	467506.686670	38.251226
2097.274368	468357.149234	38.256244
2099.115074	469203.791224	38.261261
2101.678739	470050.024313	38.266279
2103.203094	470895.077843	38.271296
2105.605680	471736.462868	38.276314
2107.696306	472590.645594	38.281332
2109.640596	473445.925686	38.286349
2112.199514	474306.067557	38.291367
2114.231461	475148.726755	38.296384
2115.936859	476016.711393	38.301402
2117.950042	476861.317531	38.306420
2119.834738	477718.989499	38.311437
2122.139199	478572.006712	38.316455
2124.289509	479446.678094	38.321472
2126.130933	480303.479829	38.326490
2128.041044	481189.118271	38.331508
2130.218299	482070.326680	38.336525
2132.303479	482931.813170	38.341543
2134.140121	483820.870657	38.346560
2135.696757	484704.022805	38.351578
2138.126000	485590.623080	38.356596
2140.111240	486496.741324	38.361613
2142.038020	487398.784312	38.366631
2144.013676	488293.099960	38.371648
2146.177808	489165.632504	38.376666
2148.173728	490044.711811	38.381684
2150.347476	490928.412053	38.386701
2152.758556	491801.681452	38.391719
2154.429075	492686.233736	38.396736
2157.033160	493571.041208	38.401754
2158.863087	494453.104960	38.406772
2160.576791	495341.803829	38.411789
2162.328014	496228.583430	38.416807
2164.405173	497152.248854	38.421824
2166.372212	498074.520014	38.426842
2168.674955	498985.838385	38.431860
2170.442910	499921.916024	38.436877
2172.893988	500839.567187	38.441895
2175.047268	501776.890312	38.446912
2176.976385	502722.217857	38.451930
2179.460321	503658.926504	38.456948
2181.370543	504611.816025	38.461965
2183.460323	505561.594897	38.466983
2185.441876	506533.525608	38.472000
2187.684151	507492.648080	38.477018
2190.153031	508458.735962	38.482036
2191.870608	509447.982706	38.487053
2194.455938	510414.590065	38.492071
2196.801554	511397.865974	38.497088
2198.676078	512387.511004	38.502106
2200.936952	513369.217694	38.507124
2202.952512	514371.923006	38.512141
2205.325600	515345.373651	38.517159
2207.612591	516343.826452	38.522176
2210.116378	517352.107866	38.527194
2213.015657	518336.574752	38.532212
2214.602954	519337.622491	38.537229
2217.648661	520331.260771	38.542247
2220.301177	521319.105970	38.547264
2222.895389	522302.867012	38.552282
2225.335547	523284.877514	38.557300
2227.706764	524290.712845	38.562317
2230.180947	525256.823980	38.567335
2232.314136	526227.261205	38.572352
2234.522907	527219.027788	38.577370
2236.731142	528182.880171	38.582388
2239.126234	529171.415021	38.587405
2241.276706	530148.998096	38.592423
2243.542367	531115.571985	38.597440
2245.585706	532110.263049	38.602458
2248.235880	533096.530730	38.607476
2250.089457	534093.434850	38.612493
2252.266870	535074.110124	38.617511
2254.941642	536052.372465	38.622528
2257.077743	537037.703854	38.627546
2259.447144	538029.723698	38.632564
2261.459636	539032.603783	38.637581
2263.621131	540015.966193	38.642599
2265.864336	541004.933219	38.647616
2268.075302	541998.566297	38.652634
2270.618020	542980.957016	38.657652
2273.057165	543978.790549	38.662669
2275.217790	544981.277428	38.667687
2277.673601	545975.847965	38.672704
2279.709937	546971.171418	38.677722
2282.041509	547956.568508	38.682740
2284.114658	548963.058890	38.687757
2286.263042	549963.379436	38.692775
2288.531305	550962.702662	38.697792
2290.642671	551981.536482	38.702810
2292.950724	552973.617793	38.707828
2295.172966	553983.486502	38.712845
2297.648787	554976.047820	38.717863
2299.748293	555950.001810	38.722880
2301.784031	556933.897345	38.727898
2303.957179	557906.592164	38.732916
2306.250759	558893.819420	38.737933
2308.048735	559898.139283	38.742951
2310.264910	560886.739213	38.747968
2312.375693	561898.342567	38.752986
2315.266929	562902.104126	38.758004
2317.332733	563916.775258	38.763021
2319.238701	564915.221123	38.768039
2321.850697	565943.056066	38.773056
2323.871349	566978.741719	38.778074
2326.128023	567998.538243	38.783092
2328.463813	569043.548004	38.788109
2330.684917	570086.784975	38.793127
2333.049987	571142.765595	38.798144
2334.997541	572197.422818	38.803162
2337.575680	573250.383088	38.808180
2340.087269	574310.544812	38.813197
2342.407999	575369.093521	38.818215
2345.036276	576427.753699	38.823232
2347.249218	577492.916431	38.828250
2350.048098	578561.153370	38.833268
2352.484167	579627.201483	38.838285
2354.616735	580695.867099	38.843303
2357.148370	581763.120839	38.848320
2359.302093	582840.827456	38.853338
2361.598417	583922.378294	38.858356
2363.843622	585010.060568	38.863373
2366.099617	586096.842042	38.868391
2368.576672	587174.164346	38.873408
2371.157342	588284.963942	38.878426
2374.032552	589397.718444	38.883444
2376.272107	590486.565411	38.888461
2378.664754	591566.467252	38.893479
2380.818373	592668.763038	38.898496
2382.791133	593771.688359	38.903514
2385.545884	594881.998648	38.908532
2387.939171	595992.965877	38.913549
2390.305143	597114.954612	38.918567
2392.843458	598234.804219	38.923584
2395.258396	599352.062789	38.928602
2397.756097	600470.302658	38.933620
2400.465308	601591.204575	38.938637
2402.766691	602716.722176	38.943655
2405.143080	603824.694069	38.948672
2407.570732	604951.424809	38.953690
2410.065006	606061.014077	38.958708
2412.449836	607191.085754	38.963725
2414.799376	608314.945273	38.968743
2417.344772	609443.515530	38.973760
2419.557482	610571.277519	38.978778
2422.360141	611692.425194	38.983796
2424.782610	612827.081461	38.988813
2426.811483	613953.583874	38.993831
2429.517518	615084.862836	38.998848
2431.543276	616224.641170	39.003866
2434.169210	617356.952213	39.008884
2436.935333	618500.624801	39.013901
2439.236080	619633.105789	39.018919
2441.953482	620763.151550	39.023936
2444.246609	621898.749085	39.028954
2447.003881	623025.904711	39.033972
2449.352621	624160.007518	39.038989
2451.898434	625297.856846	39.044007
2454.773674	626412.097521	39.049024
2456.717719	627538.866618	39.054042
2459.241343	628633.799425	39.059060
2461.794693	629738.205748	39.064077
2464.240098	630831.127642	39.069095
2467.036439	631921.831588	39.074112
2468.948281	633010.571481	39.079130
2471.510901	634097.044584	39.084148
2473.990964	635214.722236	39.089165
2476.153652	636308.521177	39.094183
2478.752565	637404.080388	39.099200
2481.025365	638514.750614	39.104218
2483.476120	639616.389748	39.109236
2485.741995	640746.933306	39.114253
2487.929662	641879.710850	39.119271
2490.821396	643005.612480	39.124288
2492.562165	644150.036586	39.129306
2495.137808	645282.872903	39.134324
2498.053888	646434.378348	39.139341
2500.089370	647590.535793	39.144359
2502.890946	648739.255068	39.149376
2505.087721	649908.333448	39.154394
2507.452594	651072.014118	39.159412
2510.252501	652241.518850	39.164429
2512.713098	653422.703943	39.169447
2515.329100	654598.790046	39.174464
2517.171157	655781.441157	39.179482
2519.866419	656971.133548	39.184500
2522.623651	658169.289687	39.189517
2524.787739	659373.424041	39.194535
2527.419924	660582.462598	39.199552
2529.757190	661793.391750	39.204570
2532.400801	663010.741446	39.209588
2535.352594	664222.511081	39.214605
2537.354586	665432.592951	39.219623
2539.975879	666642.370958	39.224640
2542.652164	667888.861569	39.229658
2545.243938	669122.316888	39.234676
2547.913424	670352.067626	39.239693
2550.316348	671599.362030	39.244711
2553.126522	672834.637497	39.249728
2555.762269	674079.477469	39.254746
2558.170296	675312.654438	39.259764
2560.816856	676560.743929	39.264781
2563.264411	677814.764247	39.269799
2566.142640	679068.992138	39.274816
2568.386977	680329.566003	39.279834
2571.175195	681580.139299	39.284852
2573.785524	682839.167600	39.289869
2575.901062	684103.668830	39.294887
2578.939825	685365.955988	39.299904
2581.577015	686633.200482	39.304922
2583.993338	687893.899391	39.309940
2586.912661	689152.155699	39.314957
2589.010457	690437.774719	39.319975
2591.886640	691694.790253	39.324992
2594.387326	692964.049181	39.330010
2596.927182	694236.148657	39.335028
2599.773712	695524.934596	39.340045
2602.380200	696802.957625	39.345063
2605.282529	698074.051802	39.350080
2607.984590	699351.294422	39.355098
2610.244063	700627.879410	39.360116
2612.660913	701901.873184	39.365133
2615.234632	703181.356332	39.370151
2617.705669	704461.313124	39.375168
2620.041083	705764.890777	39.380186
2622.396995	707053.057681	39.385204
2625.381147	708342.861128	39.390221
2627.538664	709644.743413	39.395239
2630.219273	710906.820190	39.400256
2633.290662	712177.312263	39.405274
2635.840791	713428.391500	39.410292
2638.434905	714673.734963	39.415309
2641.065692	715932.699157	39.420327
2643.610451	717195.102755	39.425344
2645.896485	718466.810967	39.430362
2648.891812	719735.092849	39.435380
2651.692246	721005.836501	39.440397
2654.151964	722286.829372	39.445415
2656.952532	723566.975456	39.450432
2659.119241	724842.281797	39.455450
2661.481159	726138.369892	39.460468
2664.451491	727428.914495	39.465485
2666.642325	728745.281487	39.470503
2669.332393	730048.457897	39.475520
2671.972530	731360.870944	39.480538
2674.506119	732682.969375	39.485556
2677.337097	734020.015180	39.490573
2679.570728	735353.876805	39.495591
2682.251047	736683.494355	39.500608
2684.984083	738032.628987	39.505626
2687.822370	739392.426728	39.510644
2690.668979	740750.757847	39.515661
2693.007759	742109.236884	39.520679
2695.773142	743467.363696	39.525696
2698.115065	744845.105210	39.530714
2700.764902	746235.869795	39.535732
2703.527149	747609.754034	39.540749
2706.164064	749005.206705	39.545767
2708.956709	750390.033976	39.550784
2711.901510	751799.031696	39.555802
2714.082085	753205.632983	39.560820
2717.123526	754614.792078	39.565837
2719.868162	756028.962960	39.570855
2722.600466	757429.629321	39.575872
2725.470996	758851.088345	39.580890
2728.376720	760282.466044	39.585908
2731.094260	761702.089113	39.590925
2734.115920	763116.918477	39.595943
2737.371865	764532.329772	39.600960
2740.190580	765957.236847	39.605978
2742.653797	767368.555717	39.610996
2745.848293	768782.487109	39.616013
2748.742299	770195.413366	39.621031
2751.584867	771621.300735	39.626048
2754.312479	773028.799962	39.631066
2757.171885	774440.431003	39.636084
2760.105685	775859.736745	39.641101
2762.445166	777272.874290	39.646119
2765.680573	778701.303919	39.651136
2769.085562	780107.825011	39.656154
2771.541791	781527.973513	39.661172
2774.659157	782938.067256	39.666189
2777.388769	784351.678438	39.671207
2780.186492	785738.658689	39.676224
2783.142285	787147.954536	39.681242
2785.773792	788544.277102	39.686260
2788.566730	789953.438570	39.691277
2791.243156	791364.055529	39.696295
2794.252396	792768.799259	39.701312
2797.211742	794175.868751	39.706330
2800.125359	795589.179917	39.711348
2802.683056	796987.376428	39.716365
2805.343354	798388.851390	39.721383
2808.230087	799799.701109	39.726400
2810.972704	801211.267444	39.731418
2813.127011	802613.247585	39.736436
2816.027323	803975.091675	39.741453
2818.619788	805350.414451	39.746471
2821.677120	806723.184621	39.751488
2824.235245	808101.532051	39.756506
2826.657418	809481.823840	39.761524
2829.776910	810861.916611	39.766541
2832.696712	812246.844166	39.771559
2835.573423	813620.355924	39.776576
2838.231492	815019.269648	39.781594
2840.785537	816419.814520	39.786612
2843.583608	817816.316041	39.791629
2846.236278	819236.861218	39.796647
2848.793354	820659.901693	39.801664
2852.158874	822070.793331	39.806682
2854.590748	823504.907171	39.811700
2857.224307	824930.775085	39.816717
2860.198007	826381.636241	39.821735
2862.965028	827832.747393	39.826752
2865.621761	829292.524022	39.831770
2868.265513	830770.933308	39.836788
2871.347377	832224.866476	39.841805
2873.788738	833709.607822	39.846823
2876.464708	835182.233403	39.851840
2879.599989	836669.783729	39.856858
2882.353688	838173.505379	39.861876
2885.170150	839669.807528	39.866893
2887.972441	841176.805959	39.871911
2890.634021	842685.903143	39.876928
2893.610352	844214.722727	39.881946
2896.296777	845741.956739	39.886964
2899.598305	847270.761220	39.891981
2902.026611	848815.277012	39.896999
2904.792608	850353.721115	39.902016
2907.907822	851909.117262	39.907034
2910.791173	853473.583579	39.912052
2913.546559	855029.909446	39.917069
2916.515129	856602.795735	39.922087
2919.306822	858167.061534	39.927104
2922.114648	859746.158659	39.932122
2924.983970	861334.247205	39.937140
2928.049376	862925.187592	39.942157
2930.958444	864522.039385	39.947175
2933.873826	866116.919432	39.952192
2937.056557	867707.459415	39.957210
2939.887425	869298.994031	39.962228
2942.790333	870894.937450	39.967245
2945.885162	872517.144795	39.972263
2948.892591	874117.826313	39.977280
2952.304769	875717.817253	39.982298
2955.029506	877313.427161	39.987316
2958.534754	878916.698363	39.992333
2961.666240	880530.520301	39.997351
2964.368341	882128.601505	40.002368
2967.938104	883711.609329	40.007386
2971.349182	885312.182437	40.012404
2974.288751	886901.962775	40.017421
2977.119638	888499.821921	40.022439
2980.222472	890085.998090	40.027456
2983.186176	891659.409133	40.032474
2986.144003	893253.228190	40.037492
2989.277013	894843.488829	40.042509
2991.891316	896435.513332	40.047527
2994.717607	898029.660326	40.052544
2997.985076	899610.374237	40.057562
3001.047446	901213.222947	40.062580
3004.198721	902802.792457	40.067597
3007.180719	904394.347484	40.072615
3010.437196	905971.448503	40.077632
3013.653541	907518.761632	40.082650
3016.358903	909051.779998	40.087668
3019.450965	910585.369431	40.092685
3022.731452	912116.868542	40.097703
3025.478018	913658.700163	40.102720
3028.128381	915192.236027	40.107738
3030.684967	916741.113815	40.112756
3033.920480	918275.227381	40.117773
3036.536612	919827.445959	40.122791
3039.483591	921395.004552	40.127808
3042.414998	922968.061835	40.132826
3045.346243	924540.181706	40.137844
3048.442346	926116.035420	40.142861
3051.115071	927714.793691	40.147879
3053.934137	929315.734271	40.152896
3056.864822	930916.176457	40.157914
3059.578417	932522.303518	40.162932
3062.542216	934149.257018	40.167949
3065.520796	935795.906091	40.172967
3068.240667	937445.241599	40.177984
3071.480358	939087.564321	40.183002
3074.089023	940751.090127	40.188020
3076.873979	942417.976987	40.193037
3080.164304	944090.363794	40.198055
3083.415987	945779.798182	40.203072
3086.603905	947472.607385	40.208090
3089.582901	949161.935393	40.213108
3092.250702	950863.454312	40.218125
3095.477242	952572.331271	40.223143
3098.238357	954302.556392	40.228160
3101.454682	956050.937261	40.233178
3104.483397	957823.065329	40.238196
3107.686834	959607.527763	40.243213
3110.839795	961397.995735	40.248231
3113.787081	963197.908832	40.253248
3117.118549	964983.421649	40.258266
3119.694171	966795.751992	40.263284
3123.137068	968607.661025	40.268301
3126.269939	970417.878340	40.273319
3129.015324	972246.418992	40.278336
3132.116432	974053.932916	40.283354
3135.475714	975890.280694	40.288372
3138.565018	977723.452063	40.293389
3141.900519	979552.195084	40.298407
3144.675580	981414.539162	40.303424
3147.858691	983243.683911	40.308442
3150.708145	985100.333486	40.313460
3153.916845	986956.416503	40.318477
3157.052316	988827.569507	40.323495
3160.234886	990694.890162	40.328512
3163.121081	992562.813008	40.333530
3166.280192	994441.544951	40.338548
3169.367988	996324.621732	40.343565
3172.755946	998208.189265	40.348583
3175.344251	1000099.223835	40.353600
3178.927928	1001995.189271	40.358618
3182.177806	1003900.567797	40.363636
3185.337187	1005799.305186	40.368653
3188.730156	1007686.796813	40.373671
3191.838668	1009604.623861	40.378688
3195.592961	1011488.747513	40.383706
3198.676497	1013381.553177	40.388724
3201.600556	1015275.491267	40.393741
3205.181921	1017171.393315	40.398759
3208.380524	1019069.718069	40.403776
3211.759602	1020959.825738	40.408794
3214.980687	1022854.350558	40.413812
3218.060483	1024714.617622	40.418829
3221.433868	1026556.823540	40.423847
3224.296067	1028399.569333	40.428864
3227.792386	1030232.331937	40.433882
3230.944363	1032067.831818	40.438900
3234.148996	1033919.125374	40.443917
3237.238272	1035757.087957	40.448935
3240.347683	1037608.328474	40.453952
3243.573092	1039442.254410	40.458970
3246.560786	1041298.071024	40.463988
3249.514668	1043158.668490	40.469005
3252.589200	1045023.245280	40.474023
3255.478302	1046916.784336	40.479040
3258.761061	1048794.499905	40.484058
3261.610574	1050697.147210	40.489076
3264.580669	1052602.582488	40.494093
3267.980385	1054512.674124	40.499111
3270.697873	1056442.113224	40.504128
3273.950696	1058389.044786	40.509146
3276.841578	1060342.071242	40.514164
3279.733412	1062310.726977	40.519181
3283.470854	1064267.980724	40.524199
3286.356383	1066248.759772	40.529216
3289.565223	1068233.758037	40.534234
3293.399386	1070231.357302	40.539252
3295.988143	1072235.046157	40.544269
3299.620260	1074238.691819	40.549287
3302.338800	1076259.758465	40.554304
3305.830366	1078282.151875	40.559322
3308.945405	1080323.188964	40.564340
3312.273012	1082363.618179	40.569357
3315.907542	1084401.606663	40.574375
3318.845683	1086454.336636	40.579392
3322.531235	1088516.392692	40.584410
3325.942019	1090582.677844	40.589428
3328.798398	1092650.558787	40.594445
3332.603612	1094716.635397	40.599463
3335.602536	1096787.208365	40.604480
3339.050484	1098879.327272	40.609498
3342.557528	1100957.374655	40.614516
3345.533479	1103049.194872	40.619533
3349.103998	1105143.535113	40.624551
3352.262631	1107248.651053	40.629568
3355.515409	1109353.403915	40.634586
3358.660295	1111448.691814	40.639604
3362.194482	1113561.930445	40.644621
3365.769378	1115670.717049	40.649639
3368.543152	1117799.999200	40.654656
3372.123939	1119927.256649	40.659674
3375.130364	1122063.923465	40.664692
3378.434303	1124209.653803	40.669709
3381.540880	1126356.261921	40.674727
3384.650299	1128523.820137	40.679744
3388.164962	1130667.675463	40.684762
3391.620288	1132830.862722	40.689780
3394.876235	1134988.181583	40.694797
3398.421991	1137164.366933	40.699815
3401.691663	1139345.573316	40.704832
3404.890536	1141511.606488	40.709850
3408.277152	1143682.585960	40.714868
3411.474631	1145873.881381	40.719885
3415.011335	1148056.179378	40.724903
3418.109224	1150240.858441	40.729920
3421.507383	1152430.247536	40.734938
3424.913066	1154642.980435	40.739956
3428.570438	1156834.929289	40.744973
3432.054288	1159029.386794	40.749991
3435.635840	1161218.197302	40.755008
3439.021019	1163387.495786	40.760013
3442.597264	1165509.356124	40.765018
3445.579710	1167583.731615	40.770023
3449.150123	1169568.590992	40.775028
3452.119263	1171497.619346	40.780032
3454.996571	1173352.691452	40.785037
3458.232861	1175121.181495	40.790042
3460.980737	1176816.790008	40.795047
3463.762416	1178441.668050	40.800052
3466.426780	1179987.337386	40.805056
3468.819636	1181445.703732	40.810061
3471.897677	1182832.493494	40.815066
3473.858118	1184167.442569	40.820071
3476.277010	1185418.819700	40.825076
3478.786210	1186603.767589	40.830080
3480.460301	1187712.705642	40.835085
3482.778433	1188751.267282	40.840090
3484.693047	1189734.329084	40.845095
3486.459786	1190650.040376	40.850100
3488.500088	1191516.030811	40.855104
3490.039804	1192318.174055	40.860109
3491.964730	1193063.680162	40.865114
3492.966536	1193760.396020	40.870119
3494.974553	1194397.412839	40.875124
3495.985731	1194990.011145	40.880128
3497.486261	1195527.165258	40.885133
3498.659748	1196041.037151	40.890138
3499.626585	1196495.101360	40.895143
3501.239041	1196911.477137	40.900148
3502.488997	1197288.274949	40.905152
3503.462077	1197623.331016	40.910157
3504.557111	1197926.722214	40.915162
3505.122595	1198193.025341	40.920167
3506.486519	1198430.565798	40.925172
3507.112823	1198650.202616	40.930176
3507.994625	1198819.687984	40.935181
3508.741579	1198957.948621	40.940186
3509.477088	1199086.075325	40.945191
3510.372284	1199185.559349	40.950196
3510.831052	1199250.777950	40.955200
3511.316726	1199288.316794	40.960205
3512.036606	1199327.599211	40.965210
3512.303424	1199332.621120	40.970215
3512.671812	1199318.864022	40.975220
3513.320518	1199297.180527	40.980224
3513.803860	1199241.751625	40.985229
3514.530628	1199177.369706	40.990234
3514.897141	1199111.170006	40.995239
3515.321332	1199024.320279	41.000244
3515.638766	1198919.285851	41.005248
3515.904999	1198773.070244	41.010253
3516.501856	1198638.242568	41.015258
3516.512187	1198495.345053	41.020263
3517.385059	1198325.747803	41.025268
3517.361511	1198162.860886	41.030272
3517.462883	1197973.298866	41.035277
3517.919733	1197776.445675	41.040282
3517.835100	1197582.770961	41.045287
3518.590599	1197358.074940	41.050292
3518.760781	1197135.905650	41.055296
3518.947110	1196911.190020	41.060301
3519.058457	1196683.285710	41.065306
3519.303186	1196440.424995	41.070311
3519.462747	1196185.927160	41.075316
3519.531535	1195938.753812	41.080320
3519.636788	1195672.317647	41.085325
3519.734075	1195400.611576	41.090330
3519.726148	1195127.030748	41.095335
3520.174791	1194849.698382	41.100340
3520.154401	1194571.771059	41.105344
3520.547385	1194282.586193	41.110349
3520.479772	1193978.059938	41.115354
3520.422792	1193690.794168	41.120359
3520.905350	1193377.126066	41.125364
3520.882383	1193081.837594	41.130368
3521.135471	1192758.589308	41.135373
3521.156486	1192445.410239	41.140378
3521.188300	1192126.010180	41.145383
3521.139952	1191796.551071	41.150388
3521.165365	1191480.306363	41.155392
3521.189210	1191148.445147	41.160397
3521.362872	1190835.613076	41.165402
3521.288201	1190488.785073	41.170407
3521.518269	1190153.630917	41.175412
3521.678031	1189813.767372	41.180416
3521.608160	1189474.389249	41.185421
3521.495210	1189125.690223	41.190426
3521.346576	1188787.219920	41.195431
3521.577923	1188442.930296	41.200436
3521.740445	1188102.483735	41.205440
3521.882053	1187749.231212	41.210445
3521.890985	1187390.240670	41.215450
3521.466866	1187039.289522	41.220455
3521.707708	1186692.719041	41.225460
3521.521660	1186333.405161	41.230464
3521.843439	1185974.452975	41.235469
3521.994767	1185613.999005	41.240474
3522.139879	1185261.328569	41.245479
3522.149144	1184901.506880	41.250484
3522.034536	1184541.586517	41.255488
3521.902896	1184179.009516	41.260493
3522.038654	1183807.141924	41.265498
3521.834740	1183437.279704	41.270503
3521.586345	1183070.692165	41.275508
3521.577684	1182713.827047	41.280512
3521.700531	1182347.127212	41.285517
3522.134316	1181982.044532	41.290522
3521.794172	1181604.637983	41.295527
3521.818411	1181225.731856	41.300532
3521.768807	1180861.873802	41.305536
3521.960030	1180503.788113	41.310541
3521.838399	1180126.708855	41.315546
3521.712891	1179757.795404	41.320551
3521.932671	1179380.323218	41.325556
3522.092673	1179023.741576	41.330560
3521.668852	1178635.396301	41.335565
3521.647455	1178256.940341	41.340570
3521.452036	1177906.934197	41.345575
3521.956451	1177535.592579	41.350580
3521.668158	1177148.338552	41.355584
3521.463031	1176782.618673	41.360589
3521.389761	1176406.863202	41.365594
3521.454466	1176041.894853	41.370599
3521.523905	1175666.156618	41.375604
3521.599418	1175288.411041	41.380608
3521.350018	1174911.916876	41.385613
3521.321640	1174539.789382	41.390618
3521.365985	1174185.062962	41.395623
3521.563690	1173792.294312	41.400628
3521.335598	1173419.176880	41.405632
3521.122593	1173043.484435	41.410637
3521.363722	1172667.690109	41.415642
3521.282449	1172307.010156	41.420647
3521.408770	1171935.708471	41.425652
3521.158611	1171553.501724	41.430656
3521.050132	1171190.862713	41.435661
3521.035378	1170814.128020	41.440666
3521.095132	1170438.674552	41.445671
3521.217707	1170053.749436	41.450676
3521.012456	1169697.720905	41.455680
3520.970285	1169326.544276	41.460685
3521.143962	1168947.284864	41.465690
3520.792058	1168570.726816	41.470695
3520.895244	1168197.841721	41.475700
3520.923279	1167847.877454	41.480704
3520.872521	1167477.609020	41.485709
3521.255094	1167098.180941	41.490714
3520.822543	1166737.173751	41.495719
3520.881537	1166352.080628	41.500724
3520.895078	1165995.291580	41.505728
3520.757825	1165615.086140	41.510733
3520.773766	1165241.249061	41.515738
3520.268813	1164875.781466	41.520743
3520.551185	1164501.942113	41.525748
3520.958449	1164127.299892	41.530752
3520.748957	1163763.972773	41.535757
3520.735440	1163398.132116	41.540762
3520.445661	1163029.855180	41.545767
3520.508024	1162643.260362	41.550772
3520.282234	1162269.628719	41.555776
3520.252187	1161921.639464	41.560781
3520.309989	1161550.461048	41.565786
3519.952196	1161176.962207	41.570791
3520.171115	1160818.463330	41.575796
3520.120462	1160466.694978	41.580800
3520.028102	1160092.413529	41.585805
3520.126049	1159739.248585	41.590810
3519.776568	1159371.480532	41.595815
3520.075773	1159012.372291	41.600820
3519.985266	1158642.808746	41.605824
3519.869683	1158283.435291	41.610829
3519.895994	1157922.028060	41.615834
3519.809392	1157572.719281	41.620839
3519.762804	1157196.805191	41.625844
3519.851438	1156836.164132	41.630848
3519.894288	1156474.559974	41.635853
3520.055091	1156107.614212	41.640858
3519.608349	1155758.338662	41.645863
3519.649143	1155390.038146	41.650868
3519.838618	1155034.933291	41.655872
3519.549997	1154672.124328	41.660877
3519.663673	1154310.832728	41.665882
3519.484027	1153967.734191	41.670887
3519.689049	1153593.981369	41.675892
3519.547960	1153235.970291	41.680896
3519.631041	1152874.585091	41.685901
3519.378406	1152517.774004	41.690906
3519.471085	1152163.437825	41.695911
3519.682092	1151806.786187	41.700916
3519.376969	1151439.875454	41.705920
3519.265840	1151085.216249	41.710925
3519.242316	1150731.939104	41.715930
3519.164317	1150377.132079	41.720935
3518.844870	1150019.499806	41.725940
3518.783621	1149661.232472	41.730944
3518.903673	1149312.856192	41.735949
3519.011039	1148967.016504	41.740954
3518.923966	1148618.439011	41.745959
3518.891010	1148259.503392	41.750964
3518.878093	1147917.309368	41.755968
3519.079001	1147572.689235	41.760973
3519.150438	1147224.372508	41.765978
3518.618536	1146861.539026	41.770983
3518.698254	1146515.069338	41.775988
3518.706566	1146166.882757	41.780992
3518.665330	1145824.747257	41.785997
3518.775492	1145469.768603	41.791002
3518.497616	1145127.342540	41.796007
3518.344014	1144786.674971	41.801012
3518.543943	1144442.229852	41.806016
3518.338054	1144105.224322	41.811021
3518.451813	1143746.431695	41.816026
3518.300013	1143413.829553	41.821031
3518.180025	1143068.683864	41.826036
3518.002043	1142732.250006	41.831040
3518.003758	1142391.117947	41.836045
3518.011291	1142059.163088	41.841050
3517.959044	1141725.869307	41.846055
3518.196028	1141384.159316	41.851060
3518.218115	1141038.003999	41.856064
3518.015310	1140706.473256	41.861069
3517.950168	1140366.549890	41.866074
3517.956999	1140033.044909	41.871079
3518.003642	1139689.264331	41.876084
3517.852267	1139356.027444	41.881088
3517.792594	1139030.061885	41.886093
3518.367520	1138682.997275	41.891098
3518.219731	1138344.001708	41.896103
3518.068045	1138013.527847	41.901108
3518.076510	1137668.388495	41.906112
3517.977620	1137314.510634	41.911117
3517.832845	1136982.072703	41.916122
3517.416104	1136655.450290	41.921127
3517.391033	1136322.856382	41.926132
3517.723956	1135983.630729	41.931136
3517.416744	1135637.271724	41.936141
3517.518815	1135314.184802	41.941146
3517.304840	1134994.359362	41.946151
3517.396324	1134659.837545	41.951156
3517.395238	1134336.043234	41.956160
3517.324174	1133995.617266	41.961165
3517.265134	1133677.206834	41.966170
3517.121813	1133358.601193	41.971175
3517.052954	1133009.276402	41.976180
3517.051415	1132702.199123	41.981184
3517.365757	1132392.106464	41.986189
3516.877022	1132055.520789	41.991194
3516.783127	1131735.954493	41.996199
3517.229588	1131416.375037	42.001204
3516.733326	1131103.299525	42.006208
3516.903391	1130764.527722	42.011213
3516.928671	1130444.293897	42.016218
3516.866722	1130128.332884	42.021223
3516.520262	1129803.844020	42.026228
3516.664196	1129481.441259	42.031232
3516.551007	1129172.467256	42.036237
3516.401896	1128861.009080	42.041242
3516.541101	1128551.006619	42.046247
3516.426210	1128224.006100	42.051252
3516.248347	1127910.975587	42.056256
3516.429415	1127603.288579	42.061261
3516.087148	1127293.387333	42.066266
3515.955055	1126983.623678	42.071271
3516.073515	1126673.325145	42.076276
3515.909642	1126379.987732	42.081280
3515.492069	1126070.693674	42.086285
3516.146939	1125761.109909	42.091290
3515.890879	1125465.168614	42.096295
3516.211306	1125158.935015	42.101300
3516.177005	1124857.024215	42.106304
3516.113142	1124536.449842	42.111309
3516.174475	1124231.918599	42.116314
3515.875284	1123923.812857	42.121319
3515.902991	1123609.068301	42.126324
3516.034718	1123306.471379	42.131328
3515.594120	1123001.000757	42.136333
3515.903234	1122701.767107	42.141338
3515.935380	1122401.229539	42.146343
3515.857338	1122098.217917	42.151348
3515.694288	1121794.155809	42.156352
3515.939177	1121491.818287	42.161357
3515.700404	1121177.545612	42.166362
3515.575185	1120884.851924	42.171367
3515.701397	1120577.530523	42.176372
3515.594368	1120282.134381	42.181376
3515.320760	1119985.320736	42.186381
3515.428448	1119677.283961	42.191386
3515.347797	1119386.405838	42.196391
3515.505844	1119085.470584	42.201396
3515.154115	1118802.035395	42.206400
3515.003646	1118491.019703	42.211405
3515.432856	1118194.943641	42.216410
3514.971534	1117915.004620	42.221415
3515.299399	1117613.196393	42.226420
3515.281958	1117326.960088	42.231424
3515.223717	1117043.669305	42.236429
3515.046575	1116732.841739	42.241434
3514.691012	1116451.951101	42.246439
3514.805317	1116167.251290	42.251444
3515.240280	1115876.192798	42.256448
3514.981854	1115579.608845	42.261453
3515.272628	1115297.693370	42.266458
3515.127470	1115006.111233	42.271463
3515.146140	1114717.822979	42.276468
3515.094266	1114421.617609	42.281472
3514.787511	1114126.963382	42.286477
3514.589549	1113834.277410	42.291482
3514.650653	1113565.753140	42.296487
3515.021998	1113259.878357	42.301492
3514.359596	1112981.431095	42.306496
3514.632420	1112680.593910	42.311501
3514.604112	1112401.344514	42.316506
3514.328191	1112128.988807	42.321511
3514.508333	1111856.067239	42.326516
3514.473460	1111564.852171	42.331520
3514.287593	1111290.149692	42.336525
3514.388587	1111010.902078	42.341530
3514.140655	1110736.372297	42.346535
3514.411634	1110452.392776	42.351540
3514.231079	1110173.243403	42.356544
3514.026884	1109898.186507	42.361549
3514.223141	1109618.182878	42.366554
3514.011653	1109341.094734	42.371559
3514.386850	1109071.244205	42.376564
3514.142053	1108795.564959	42.381568
3513.763057	1108526.002158	42.386573
3514.124036	1108244.659090	42.391578
3513.894843	1107982.298555	42.396583
3513.885793	1107711.488544	42.401588
3513.574870	1107450.642887	42.406592
3513.823014	1107168.880296	42.411597
3514.058990	1106902.285312	42.416602
3513.710655	1106628.135073	42.421607
3513.683890	1106363.561730	42.426612
3513.659718	1106081.978065	42.431616
3513.606232	1105813.085097	42.436621
3513.859805	1105552.531936	42.441626
3513.692500	1105301.394709	42.446631
3513.385937	1105021.521140	42.451636
3513.357428	1104766.133781	42.456640
3513.642251	1104500.749021	42.461645
3513.440739	1104235.049208	42.466650
3513.315700	1103972.858150	42.471655
3513.760308	1103709.032033	42.476660
3513.678147	1103447.286003	42.481664
3513.504567	1103169.682713	42.486669
3513.577969	1102912.948735	42.491674
3513.181404	1102652.362425	42.496679
3513.338327	1102383.550289	42.501684
3513.271288	1102134.542245	42.506688
3513.055677	1101872.550634	42.511693
3513.310203	1101603.683569	42.516698
3513.084578	1101342.145689	42.521703
3513.217340	1101093.916863	42.526708
3513.290246	1100833.356505	42.531712
3513.006573	1100574.084914	42.536717
3513.254361	1100317.389873	42.541722
3512.964063	1100073.389776	42.546727
3512.930375	1099813.753714	42.551732
3512.907317	1099549.132010	42.556736
3512.892789	1099306.581511	42.561741
3512.626965	1099049.050302	42.566746
3512.730759	1098808.083353	42.571751
3512.855147	1098545.396160	42.576756
3512.943155	1098296.950515	42.581760
3512.696869	1098042.523776	42.586765
3512.883836	1097793.273638	42.591770
3512.617752	1097554.128767	42.596775
3512.851019	1097290.980126	42.601780
3512.713775	1097041.079202	42.606784
3512.524074	1096799.688464	42.611789
3512.752384	1096535.547359	42.616794
3512.602662	1096294.414458	42.621799
3512.428804	1096030.984583	42.626804
3512.503676	1095791.322929	42.631808
3512.339086	1095547.863108	42.636813
3512.693759	1095301.245080	42.641818
3512.330009	1095064.876586	42.646823
3512.353968	1094800.971517	42.651828
3512.272954	1094565.300145	42.656832
3512.049524	1094334.139696	42.661837
3512.458836	1094084.203563	42.666842
3512.365104	1093828.883556	42.671847
3512.150662	1093582.472390	42.676852
3512.347879	1093350.722137	42.681856
3512.429317	1093114.195152	42.686861
3512.408065	1092860.253320	42.691866
3511.917657	1092630.691410	42.696871
3512.039953	1092381.968471	42.701876
3512.074042	1092157.661059	42.706880
3511.684850	1091911.777089	42.711885
3512.139443	1091679.242802	42.716890
3512.018016	1091444.303984	42.721895
3512.094657	1091194.768122	42.726900
3511.909300	1090960.872157	42.731904
3511.599744	1090730.050877	42.736909
3512.178585	1090493.710670	42.741914
3511.927184	1090252.612726	42.746919
3511.894489	1090006.200549	42.751924
3511.905313	1089771.359027	42.756928
3511.323076	1089541.298284	42.761933
3511.794832	1089315.460302	42.766938
3511.608003	1089080.525655	42.771943
3511.541940	1088840.196527	42.776948
3511.601804	1088625.892887	42.781952
3511.354785	1088401.380630	42.786957
3511.601163	1088164.802192	42.791962
3511.358211	1087941.324101	42.796967
3511.662072	1087709.219384	42.801972
3511.354479	1087482.954495	42.806977
3510.893554	1087257.472000	42.811981
3511.296293	1087037.108285	42.816986
3511.282161	1086832.232738	42.821991
3511.427326	1086583.527687	42.826996
3511.259217	1086368.310029	42.832001
3511.285898	1086141.167509	42.837005
3511.633691	1085912.812475	42.842010
3511.186675	1085697.326649	42.847015
3510.894274	1085469.633532	42.852020
3510.990263	1085248.672736	42.857025
3511.083822	1085034.988759	42.862029
3511.269388	1084811.407218	42.867034
3510.940828	1084597.296247	42.872039
3510.917963	1084370.663141	42.877044
3510.999148	1084155.125074	42.882049
3510.977831	1083934.321966	42.887053
3511.111442	1083723.072743	42.892058
3510.969444	1083496.422849	42.897063
3510.742063	1083284.353064	42.902068
3510.684982	1083060.835454	42.907073
3510.937233	1082859.506270	42.912077
3511.213547	1082643.300811	42.917082
3510.879475	1082430.352207	42.922087
3510.698618	1082202.408054	42.927092
3510.780178	1081986.304502	42.932097
3510.907310	1081774.405257	42.937101
3511.200958	1081550.576063	42.942106
3510.758507	1081340.288490	42.947111
3510.555621	1081131.008562	42.952116
3510.510823	1080919.296237	42.957121
3510.536115	1080688.376790	42.962125
3510.524229	1080476.833732	42.967130
3510.295145	1080275.200498	42.972135
3510.390410	1080070.052265	42.977140
3510.329880	1079872.694034	42.982145
3510.452979	1079668.869443	42.987149
3510.481389	1079461.022573	42.992154
3510.221576	1079258.205283	42.997159
3510.360984	1079039.480340	43.002164
3510.408449	1078843.314627	43.007169
3510.140465	1078643.066980	43.012173
3510.431681	1078436.001527	43.017178
3510.238475	1078229.391923	43.022183
3510.069064	1078027.281814	43.027188
3510.127270	1077840.676653	43.032193
3510.257652	1077623.528219	43.037197
3510.303658	1077412.240717	43.042202
3510.132113	1077213.364633	43.047207
3510.038041	1077014.180538	43.052212
3510.295145	1076821.843701	43.057217
3510.130687	1076611.903959	43.062221
3510.206120	1076394.619694	43.067226
3509.912661	1076201.583590	43.072231
3509.829933	1076007.449743	43.077236
3509.938793	1075817.022326	43.082241
3509.717258	1075615.407638	43.087245
3510.324931	1075408.271276	43.092250
3509.849685	1075220.223975	43.097255
3509.995877	1075012.476388	43.102260
3509.878069	1074817.537744	43.107265
3509.603232	1074631.934230	43.112269
3509.500765	1074429.775966	43.117274
3509.318485	1074238.669171	43.122279
3509.704358	1074037.952797	43.127284
3509.606213	1073853.446394	43.132289
3509.468954	1073671.629897	43.137293
3509.691766	1073483.503920	43.142298
3509.439112	1073290.454301	43.147303
3509.416991	1073106.198367	43.152308
3509.881789	1072918.013093	43.157313
3509.595072	1072711.498337	43.162317
3509.921701	1072514.867161	43.167322
3509.611300	1072344.564728	43.172327
3509.726691	1072147.186465	43.177332
3509.293148	1071956.137373	43.182337
3509.513021	1071758.727894	43.187341
3509.484821	1071563.081906	43.192346
3509.546015	1071392.880848	43.197351
3509.115342	1071190.945221	43.202356
3509.518652	1071006.644629	43.207361
3509.218841	1070818.993668	43.212365
3509.429468	1070639.517977	43.217370
3509.184971	1070442.618099	43.222375
3509.013327	1070253.388772	43.227380
3509.375738	1070080.694314	43.232385
3509.232519	1069892.216816	43.237389
3509.262205	1069713.509604	43.242394
3509.256341	1069528.169242	43.247399
3509.011051	1069343.919544	43.252404
3509.348416	1069169.277769	43.257409
3508.960519	1068986.577770	43.262413
3509.144506	1068795.797388	43.267418
3508.632773	1068620.220359	43.272423
3508.866873	1068442.784129	43.277428
3509.100204	1068273.707781	43.282433
3509.077650	1068083.898196	43.287437
3508.596443	1067899.350309	43.292442
3508.235981	1067736.894189	43.297447
3508.473301	1067574.527137	43.302452
3509.033802	1067407.774395	43.307457
3508.728898	1067228.175728	43.312461
3508.955980	1067048.291209	43.317466
3508.749018	1066875.301033	43.322471
3508.833481	1066709.086364	43.327476
3508.464842	1066528.609644	43.332481
3508.604114	1066352.275640	43.337485
3508.960077	1066173.976446	43.342490
3509.027579	1066005.338462	43.347495
3508.992596	1065821.609107	43.352500
3508.604282	1065651.977159	43.357505
3508.134206	1065477.062210	43.362509
3508.800386	1065303.878689	43.367514
3508.170727	1065139.562038	43.372519
3508.331867	1064962.794962	43.377524
3508.527213	1064796.985197	43.382529
3508.351022	1064641.142155	43.387533
3508.511015	1064468.400544	43.392538
3508.300872	1064293.693742	43.397543
3508.208355	1064126.179094	43.402548
3508.427916	1063967.172461	43.407553
3508.164171	1063809.588094	43.412557
3508.618931	1063629.072882	43.417562
3508.361643	1063469.552970	43.422567
3508.323142	1063304.891562	43.427572
3508.314599	1063133.098152	43.432577
3508.194247	1062969.498872	43.437581
3508.483991	1062813.045989	43.442586
3508.207143	1062651.773044	43.447591
3508.264535	1062480.140876	43.452596
3508.285823	1062306.969144	43.457601
3508.342009	1062148.610633	43.462605
3508.294561	1061977.557620	43.467610
3508.145612	1061817.394315	43.472615
3507.967686	1061647.507741	43.477620
3508.030628	1061486.433459	43.482625
3508.102418	1061333.536523	43.487629
3508.215508	1061151.744671	43.492634
3507.954554	1061005.633006	43.497639
3507.909763	1060846.579663	43.502644
3507.868399	1060692.142976	43.507649
3507.740118	1060535.983040	43.512653
3507.942272	1060381.112356	43.517658
3508.037215	1060227.795709	43.522663
3507.744796	1060061.345659	43.527668
3508.010694	1059907.991949	43.532673
3507.848637	1059757.882492	43.537677
3507.912035	1059597.426971	43.542682
3507.795609	1059439.981993	43.547687
3507.967877	1059277.091463	43.552692
3507.463550	1059118.449111	43.557697
3507.382030	1058981.693044	43.562701
3507.484148	1058828.625206	43.567706
3507.806407	1058684.378578	43.572711
3507.710708	1058525.940821	43.577716
3507.844158	1058371.506562	43.582721
3507.903185	1058215.057278	43.587725
3507.622522	1058065.788202	43.592730
3507.760653	1057922.900641	43.597735
3507.698459	1057745.745657	43.602740
3507.689442	1057601.814272	43.607745
3507.792928	1057450.923798	43.612749
3507.505036	1057286.123296	43.617754
3507.740233	1057153.123566	43.622759
3507.626750	1056995.800931	43.627764
3507.742381	1056837.954295	43.632769
3507.177203	1056697.945112	43.637773
3507.741090	1056541.076086	43.642778
3507.114889	1056398.371247	43.647783
3507.020894	1056254.033211	43.652788
3507.570357	1056112.476459	43.657793
3507.198021	1055968.369524	43.662797
3507.351855	1055816.076828	43.667802
3507.483026	1055674.577735	43.672807
3507.261899	1055521.760415	43.677812
3507.515730	1055375.896438	43.682817
3506.717232	1055235.599386	43.687821
3507.362285	1055088.506780	43.692826
3507.068890	1054952.649471	43.697831
3507.488872	1054809.442026	43.702836
3507.503245	1054664.080628	43.707841
3507.174966	1054512.409711	43.712845
3507.179168	1054371.669285	43.717850
3507.067952	1054237.403129	43.722855
3506.977809	1054098.020872	43.727860
3506.986124	1053946.471768	43.732865
3506.664456	1053822.063546	43.737869
3506.853457	1053670.766338	43.742874
3507.168023	1053538.823329	43.747879
3506.924373	1053403.787403	43.752884
3507.141967	1053271.950405	43.757889
3506.708725	1053130.864720	43.762893
3506.843330	1052996.913585	43.767898
3506.844805	1052855.074299	43.772903
3506.776688	1052708.807176	43.777908
3506.601962	1052591.964784	43.782913
3506.659060	1052468.524397	43.787917
3506.748487	1052321.931788	43.792922
3506.725319	1052192.905281	43.797927
3506.806186	1052071.380834	43.802932
3506.751990	1051916.121642	43.807937
3506.351959	1051796.984951	43.812941
3506.799110	1051660.345968	43.817946
3506.698628	1051547.423525	43.822951
3506.899980	1051398.666143	43.827956
3506.801342	1051259.406535	43.832961
3506.877117	1051138.730495	43.837965
3506.666226	1050997.553682	43.842970
3506.611892	1050864.739464	43.847975
3506.993998	1050723.650910	43.852980
3506.954664	1050596.229643	43.857985
3506.605529	1050463.743738	43.862989
3506.646261	1050336.978575	43.867994
3506.377369	1050205.534421	43.872999
3506.271346	1050067.982492	43.878004
3506.667201	1049939.413206	43.883009
3506.528457	1049817.103566	43.888013
3506.487012	1049686.670874	43.893018
3506.442826	1049567.909912	43.898023
3506.649008	1049438.974310	43.903028
3506.387083	1049297.955468	43.908033
3506.244993	1049166.658707	43.913037
3506.405027	1049044.861717	43.918042
3506.586706	1048924.602377	43.923047
3506.293647	1048783.672045	43.928052
3506.499644	1048674.307282	43.933057
3506.210566	1048549.581929	43.938061
3506.744202	1048412.365982	43.943066
3506.611505	1048288.091492	43.948071
3506.505899	1048160.045989	43.953076
3506.423866	1048040.100387	43.958081
3506.163445	1047902.037486	43.963085
3506.218617	1047773.667031	43.968090
3506.292797	1047656.389763	43.973095
3506.266378	1047537.196228	43.978100
3506.137489	1047408.461550	43.983105
3506.394625	1047296.165550	43.988109
3506.737353	1047170.918982	43.993114
3506.395729	1047048.967658	43.998119
3506.159829	1046921.494122	44.003124
3506.404767	1046800.212939	44.008129
3506.206116	1046680.064018	44.013133
3506.466688	1046553.079431	44.018138
3506.293387	1046435.720541	44.023143
3506.132447	1046311.406329	44.028148
3505.994689	1046183.030781	44.033153
3505.906763	1046070.380603	44.038157
3505.918932	1045948.636403	44.043162
3505.864799	1045839.065405	44.048167
3505.918489	1045726.674558	44.053172
3506.120573	1045598.712246	44.058177
3505.976533	1045483.452492	44.063181
3505.888063	1045369.339852	44.068186
3505.861201	1045247.876353	44.073191
3506.058204	1045128.594192	44.078196
3506.051113	1045002.680324	44.083201
3505.610578	1044902.424366	44.088205
3506.088188	1044789.268751	44.093210
3505.871591	1044673.424708	44.098215
3505.842052	1044550.787568	44.103220
3505.756151	1044439.649023	44.108225
3505.783086	1044326.268475	44.113229
3505.730085	1044200.923402	44.118234
3505.593102	1044098.188505	44.123239
3505.508372	1043974.485356	44.128244
3505.891404	1043881.029009	44.133249
3505.303884	1043778.845304	44.138253
3505.508123	1043658.081579	44.143258
3505.817470	1043555.939224	44.148263
3505.596723	1043441.808695	44.153268
3505.642283	1043337.484219	44.158273
3505.485778	1043224.111355	44.163277
3505.602010	1043109.821902	44.168282
3505.417526	1043018.569586	44.173287
3505.962895	1042912.609266	44.178292
3505.766108	1042783.102114	44.183297
3505.640814	1042683.913310	44.188301
3506.075927	1042572.361733	44.193306
3505.910137	1042451.149671	44.198311
3505.435110	1042332.207882	44.203316
3505.969396	1042228.651545	44.208321
3505.562662	1042114.137893	44.213325
3505.833830	1042006.079976	44.218330
3505.850870	1041901.153516	44.223335
3505.440325	1041780.643429	44.228340
3505.861852	1041669.075950	44.233345
3505.687279	1041572.290888	44.238349
3505.505009	1041439.754730	44.243354
3505.415824	1041341.115722	44.248359
3505.659670	1041228.022642	44.253364
3505.447202	1041120.317030	44.258369
3505.325102	1041016.942846	44.263373
3505.587076	1040913.986646	44.268378
3505.260948	1040809.772513	44.273383
3505.190726	1040698.749714	44.278388
3505.409083	1040591.252794	44.283393
3505.324048	1040511.829405	44.288397
3505.525898	1040393.700983	44.293402
3505.555158	1040289.225266	44.298407
3505.387993	1040175.985179	44.303412
3505.508636	1040080.188590	44.308417
3505.140067	1039971.616581	44.313421
3505.675313	1039857.771077	44.318426
3505.176266	1039774.249324	44.323431
3505.381663	1039657.941083	44.328436
3505.458735	1039559.822988	44.333441
3505.275456	1039450.726999	44.338445
3505.105510	1039356.415670	44.343450
3505.408023	1039243.369201	44.348455
3505.488281	1039139.443441	44.353460
3505.464480	1039030.022937	44.358465
3505.084564	1038936.029054	44.363469
3505.222137	1038846.298451	44.368474
3505.089422	1038744.623770	44.373479
3505.216638	1038639.520885	44.378484
3505.429438	1038541.749159	44.383489
3504.713019	1038443.935405	44.388493
3505.166485	1038336.936227	44.393498
3505.263411	1038236.857961	44.398503
3504.934923	1038139.168308	44.403508
3505.000214	1038035.031010	44.408513
3504.525975	1037943.356261	44.413517
3505.211964	1037848.298266	44.418522
3504.826241	1037763.760752	44.423527
3504.936614	1037660.962655	44.428532
3505.087717	1037565.117716	44.433537
3504.985867	1037470.956566	44.438541
3505.130242	1037375.496241	44.443546
3505.348048	1037280.602362	44.448551
3504.976826	1037179.325126	44.453556
3504.826085	1037072.594552	44.458561
3504.774696	1036984.702337	44.463565
3504.908826	1036887.107895	44.468570
3504.752770	1036790.719991	44.473575
3504.687055	1036705.243336	44.478580
3504.808609	1036610.353883	44.483585
3504.848552	1036516.830185	44.488589
3504.575336	1036416.490010	44.493594
3504.725829	1036334.647074	44.498599
3504.695109	1036245.192375	44.503604
3505.155966	1036147.918020	44.508609
3504.976609	1036058.388085	44.513613
3504.739775	1035963.740072	44.518618
3504.667572	1035880.573075	44.523623
3504.723621	1035800.575533	44.528628
3505.227599	1035702.705974	44.533633
3504.770389	1035600.930544	44.538637
3504.903662	1035502.344718	44.543642
3504.775675	1035417.051991	44.548647
3504.625586	1035322.088595	44.553652
3504.757364	1035220.209198	44.558657
3504.506185	1035150.893419	44.563661
3504.503846	1035059.964006	44.568666
3504.510810	1034983.058313	44.573671
3504.422662	1034882.853478	44.578676
3504.742200	1034793.704723	44.583681
3504.579714	1034718.177632	44.588685
3504.661052	1034631.580770	44.593690
3505.067102	1034538.544002	44.598695
3504.907440	1034436.504787	44.603700
3504.327950	1034345.078287	44.608705
3504.398363	1034267.184791	44.613709
3504.433801	1034183.103978	44.618714
3504.460289	1034102.119412	44.623719
3504.242551	1034006.660970	44.628724
3504.493320	1033925.249883	44.633729
3504.155768	1033844.902063	44.638733
3504.415927	1033758.745964	44.643738
3504.465772	1033682.589316	44.648743
3504.511386	1033601.400808	44.653748
3504.588702	1033510.432987	44.658753
3504.350489	1033431.611028	44.663757
3504.406793	1033341.418012	44.668762
3504.559479	1033267.367573	44.673767
3504.349284	1033186.311916	44.678772
3504.543550	1033087.189478	44.683777
3504.322729	1033000.326729	44.688781
3504.450227	1032920.953462	44.693786
3504.665570	1032837.306578	44.698791
3504.467220	1032738.629701	44.703796
3504.389794	1032670.899609	44.708801
3504.326443	1032589.036872	44.713805
3504.770185	1032494.798472	44.718810
3504.477964	1032406.583320	44.723815
3504.224707	1032333.555148	44.728820
3504.549724	1032248.526424	44.733825
3504.499096	1032169.946075	44.738829
3504.398671	1032066.111569	44.743834
3504.410949	1031993.906293	44.748839
3504.255445	1031904.208856	44.753844
3504.216863	1031832.880977	44.758849
3504.313520	1031757.077483	44.763853
3504.411407	1031681.369550	44.768858
3504.468679	1031600.827546	44.773863
3504.320135	1031514.316916	44.778868
3504.201818	1031419.281762	44.783873
3504.161801	1031346.205535	44.788877
3504.078582	1031276.136278	44.793882
3503.988667	1031192.999018	44.798887
3504.166531	1031128.208998	44.803892
3504.142701	1031035.184599	44.808897
3503.714534	1030966.910751	44.813901
3503.975987	1030889.906667	44.818906
3504.144427	1030820.758313	44.823911
3503.834901	1030740.457918	44.828916
3503.784540	1030670.956506	44.833921
3504.021177	1030593.952428	44.838925
3504.305030	1030513.744667	44.843930
3504.194611	1030429.631276	44.848935
3503.792899	1030360.183861	44.853940
3504.019775	1030274.753972	44.858945
3503.919734	1030209.902249	44.863949
3504.349841	1030143.510158	44.868954
3504.211120	1030055.522990	44.873959
3503.888297	1029983.927824	44.878964
3504.429016	1029912.770459	44.883969
3504.021629	1029832.957239	44.888973
3504.353385	1029753.408448	44.893978
3504.131092	1029671.722729	44.898983
3503.927503	1029606.493737	44.903988
3504.531318	1029518.859963	44.908993
3504.120389	1029448.337575	44.913997
3504.325795	1029359.798604	44.919002
3503.926722	1029287.335557	44.924007
3504.013636	1029220.408016	44.929012
3504.218775	1029140.774521	44.934017
3503.991559	1029065.568843	44.939021
3504.022382	1028988.479692	44.944026
3504.227429	1028915.524960	44.949031
3504.285553	1028845.789276	44.954036
3504.333857	1028755.620284	44.959041
3503.903390	1028673.179487	44.964045
3504.154615	1028596.629703	44.969050
3504.051816	1028538.247748	44.974055
3503.873788	1028462.735305	44.979060
3504.082058	1028374.761349	44.984065
3503.894577	1028304.090849	44.989069
3504.143936	1028231.023031	44.994074
3503.938809	1028171.395004	44.999079
3503.877429	1028087.528813	45.004084
3504.102625	1028007.585302	45.009089
3503.694792	1027951.668879	45.014093
3503.820872	1027870.190000	45.019098
3504.087021	1027799.147820	45.024103
3503.855821	1027715.594598	45.029108
3503.826908	1027642.371195	45.034113
3503.733802	1027578.456399	45.039117
3503.622944	1027505.147830	45.044122
3503.748902	1027442.164054	45.049127
3503.607662	1027364.209031	45.054132
3503.658917	1027299.976670	45.059137
3503.886263	1027239.008162	45.064141
3503.671024	1027163.968643	45.069146
3503.193753	1027100.789757	45.074151
3503.352127	1027047.870954	45.079156
3503.902232	1026979.484058	45.084161
3503.313145	1026908.183918	45.089165
3503.552795	1026836.746374	45.094170
3503.342852	1026780.494997	45.099175
3503.442965	1026728.551552	45.104180
3503.635064	1026653.631851	45.109185
3503.277208	1026600.793842	45.114189
3503.703014	1026538.622437	45.119194
3503.561550	1026477.028190	45.124199
3503.505048	1026406.699650	45.129204
3503.491516	1026344.501564	45.134209
3503.463294	1026280.367467	45.139213
3503.603602	1026208.066276	45.144218
3503.547876	1026150.620502	45.149223
3503.414241	1026085.338860	45.154228
3503.704645	1026020.374182	45.159233
3503.940058	1025952.414137	45.164237
3503.508926	1025887.663648	45.169242
3503.954496	1025824.318333	45.174247
3503.409493	1025769.274701	45.179252
3503.863825	1025695.267937	45.184257
3503.527424	1025625.944649	45.189261
3503.833745	1025567.270476	45.194266
3503.835720	1025494.982855	45.199271
3503.343919	1025421.128295	45.204276
3503.625704	1025351.893598	45.209281
3503.511457	1025294.836285	45.214285
3503.605179	1025233.286507	45.219290
3503.769496	1025174.631608	45.224295
3503.489498	1025108.781236	45.229300
3503.562267	1025028.626439	45.234305
3503.197595	1024982.848577	45.239309
3503.175291	1024917.922609	45.244314
3502.713883	1024860.142754	45.249319
3502.762826	1024812.163317	45.254324
3503.142986	1024745.909207	45.259329
3503.045419	1024714.912905	45.264333
3502.979948	1024646.405076	45.269338
3503.261178	1024579.971467	45.274343
3503.228645	1024514.848675	45.279348
3503.132124	1024465.921054	45.284353
3503.237978	1024425.876233	45.289357
3503.615234	1024352.252095	45.294362
3503.593805	1024288.287883	45.299367
3502.907179	1024233.349364	45.304372
3503.122163	1024173.124870	45.309377
3503.250138	1024124.738832	45.314381
3503.436300	1024063.064038	45.319386
3502.968542	1024011.964307	45.324391
3503.257254	1023955.117743	45.329396
3503.449253	1023891.792340	45.334401
3503.238389	1023833.669828	45.339405
3503.219033	1023774.739728	45.344410
3503.512359	1023719.731693	45.349415
3503.166435	1023647.186710	45.354420
3503.114173	1023586.127529	45.359425
3502.959271	1023549.802866	45.364429
3503.134659	1023495.296723	45.369434
3503.186642	1023440.422630	45.374439
3503.115392	1023376.747018	45.379444
3503.305320	1023324.078621	45.384449
3503.134734	1023274.571155	45.389453
3503.348070	1023215.209088	45.394458
3503.255946	1023161.907041	45.399463
3503.349826	1023102.078745	45.404468
3503.631752	1023040.473864	45.409473
3503.441679	1022977.007163	45.414477
3503.360078	1022919.532477	45.419482
3503.282780	1022857.500024	45.424487
3503.139864	1022802.360943	45.429492
3503.308836	1022737.959873	45.434497
3502.929613	1022683.828026	45.439501
3503.006533	1022626.808974	45.444506
3502.997913	1022596.077137	45.449511
3502.887856	1022531.040990	45.454516
3503.126437	1022473.315088	45.459521
3503.237319	1022434.806452	45.464525
3503.234741	1022378.573596	45.469530
3502.909223	1022316.963855	45.474535
3502.747366	1022265.022135	45.479540
3502.971269	1022215.149459	45.484545
3502.561451	1022178.276136	45.489549
3502.935353	1022140.788698	45.494554
3503.117157	1022077.541430	45.499559
3502.768966	1022013.992895	45.504564
3503.216680	1021971.256284	45.509569
3502.916836	1021927.963734	45.514573
3502.678228	1021869.049693	45.519578
3502.648566	1021812.330799	45.524583
3502.526871	1021771.140908	45.529588
3503.162171	1021720.129459	45.534593
3502.915718	1021670.814239	45.539597
3502.819664	1021618.564787	45.544602
3503.172698	1021569.537811	45.549607
3503.057492	1021518.842078	45.554612
3503.068096	1021469.773660	45.559617
3502.831010	1021411.824262	45.564621
3503.005557	1021367.091646	45.569626
3503.084465	1021314.907519	45.574631
3502.645389	1021266.784141	45.579636
3503.024627	1021215.325412	45.584641
3502.610547	1021179.028052	45.589645
3502.902511	1021124.770584	45.594650
3502.370968	1021085.970586	45.599655
3502.343147	1021043.790119	45.604660
3503.148864	1020988.282985	45.609665
3502.665683	1020943.558341	45.614669
3502.893344	1020890.278990	45.619674
3502.960412	1020844.590107	45.624679
3502.949518	1020797.361983	45.629684
3503.115681	1020745.061200	45.634689
3503.172918	1020700.536556	45.639693
3502.863342	1020650.737835	45.644698
3502.860170	1020582.654952	45.649703
3502.601464	1020532.943791	45.654708
3503.101513	1020489.702351	45.659713
3502.924468	1020445.408243	45.664717
3503.114232	1020388.735793	45.669722
3502.767463	1020334.478895	45.674727
3502.760691	1020292.774261	45.679732
3502.881586	1020238.439408	45.684737
3502.780041	1020198.107560	45.689741
3502.648807	1020141.291495	45.694746
3502.605607	1020116.856312	45.699751
3502.190684	1020073.665373	45.704756
3502.747660	1020021.002491	45.709761
3502.597021	1019992.607655	45.714765
3502.855458	1019941.739123	45.719770
3502.797968	1019887.624247	45.724775
3502.396450	1019844.720327	45.729780
3502.794473	1019799.453415	45.734785
3502.430385	1019757.706653	45.739789
3502.459880	1019708.134708	45.744794
3502.542516	1019662.724637	45.749799
3502.337283	1019611.444471	45.754804
3502.648969	1019590.731636	45.759809
3502.366193	1019542.179683	45.764813
3502.563096	1019481.228736	45.769818
3502.792204	1019374.096944	45.774823
3502.427075	1019225.056229	45.779828
3502.774475	1018997.217237	45.784833
3502.575915	1018711.539533	45.789837
3502.578543	1018360.032280	45.794842
3502.610072	1017940.867905	45.799847
3502.244731	1017467.492840	45.804852
3502.201472	1016930.167146	45.809857
3501.990513	1016338.950244	45.814861
3502.121077	1015657.922306	45.819866
3502.228320	1014935.070101	45.824871
3502.105061	1014135.456866	45.829876
3501.973518	1013242.795560	45.834881
3501.621599	1012309.040860	45.839885
3501.555126	1011297.853771	45.844890
3501.543795	1010211.951254	45.849895
3501.103973	1009039.999287	45.854900
3500.983719	1007801.359591	45.859905
3500.953279	1006496.609679	45.864909
3500.737471	1005086.945483	45.869914
3500.487195	1003612.148098	45.874919
3500.206707	1002058.251560	45.879924
3500.058025	1000424.969705	45.884929
3499.688528	998717.939385	45.889933
3499.341486	996928.191568	45.894938
3499.247255	995053.564637	45.899943
3499.059937	993089.841419	45.904948
3498.719670	991052.539191	45.909953
3497.997183	988926.500257	45.914957
3497.640688	986716.381262	45.919962
3497.471733	984431.680460	45.924967
3497.394419	982073.204117	45.929972
3497.058534	979591.000352	45.934977
3496.539444	977055.265640	45.939981
3495.892469	974437.761316	45.944986
3496.034369	971727.954568	45.949991
3495.425884	968931.255437	45.954996
3494.689002	966070.252235	45.960001
3494.746996	963112.075013	45.965005
3493.907131	960068.226356	45.970010
3493.653745	956942.546069	45.975015
3492.972870	953768.067371	45.980020
3492.828485	950558.709838	45.985025
3491.975776	947278.608415	45.990029
3491.658868	943902.235839	45.995034
3491.125337	940456.678852	46.000039
3490.396560	936933.753245	46.005044
3489.830624	933320.395475	46.010049
3489.134029	929634.454336	46.015053
3488.801731	925850.910549	46.020058
3487.930960	922009.369390	46.025063
3487.102762	918078.243566	46.030068
3486.497632	914056.947200	46.035073
3485.592098	909967.668517	46.040077
3484.964755	905803.721781	46.045082
3484.424252	901559.590499	46.050087
3483.652158	897223.963082	46.055092
3483.378335	892800.118584	46.060097
3482.133577	888310.293776	46.065101
3481.140725	883727.138233	46.070106
3480.763264	879065.531811	46.075111
3479.344506	874329.964425	46.080116
3478.617057	869512.340331	46.085121
3477.888300	864613.491063	46.090125
3477.124493	859631.613632	46.095130
3475.978135	854576.341055	46.100135
3475.084883	849432.430469	46.105140
3474.234799	844190.579634	46.110145
3473.200044	838895.425879	46.115149
3472.470523	833501.244350	46.120154
3471.322233	828017.735526	46.125159
3470.384680	822469.917519	46.130164
3469.425557	816847.786390	46.135169
3467.974548	811138.405298	46.140173
3467.038257	805335.025494	46.145178
3466.212173	799451.725479	46.150183
3465.214404	793481.489462	46.155188
3464.363209	787436.995568	46.160193
3462.840710	781309.699686	46.165197
3461.844079	775098.234255	46.170202
3460.916631	768789.327531	46.175207
3459.654694	762417.807557	46.180212
3458.653584	755955.059146	46.185217
3457.244387	749423.680571	46.190221
3455.956349	742786.700915	46.195226
3454.650701	736081.935681	46.200231
3453.297201	729283.699711	46.205236
3452.204298	722416.448521	46.210241
3450.617960	715464.701385	46.215245
3449.532030	708395.705492	46.220250
3448.329094	701289.060334	46.225255
3446.573604	694089.634128	46.230260
3445.393822	686810.668872	46.235265
3443.950104	679439.519536	46.240269
3442.449216	671996.943428	46.245274
3441.229289	664468.512910	46.250279
3439.136568	656867.475968	46.255284
3438.167909	649186.163721	46.260289
3436.501939	641428.573676	46.265293
3434.919491	633590.481838	46.270298
3433.599498	625676.924277	46.275303
3431.938099	617682.658727	46.280308
3430.354566	609604.722780	46.285313
3428.743819	601459.366607	46.290317
3426.914713	593230.400477	46.295322
3425.451171	584919.868507	46.300327
3423.295586	576543.429745	46.305332
3421.628807	568099.406320	46.310337
3419.917243	559563.080627	46.315341
3418.290022	550950.600397	46.320346
3416.343012	542272.902986	46.325351
3414.166447	533529.723762	46.330356
3412.700075	524701.877744	46.335361
3410.820037	515797.767596	46.340365
3408.793897	506835.552963	46.345370
3406.862794	497803.549553	46.350375
3404.770162	488689.225310	46.355380
3402.822879	479496.748197	46.360385
3400.437671	470250.309056	46.365389
3398.237904	460951.449438	46.370394
3396.484282	451568.818836	46.375399
3394.145982	442116.888261	46.380404
3391.994241	432603.977849	46.385409
3389.693776	423040.058323	46.390413
3387.447641	413390.794946	46.395418
3385.187063	403671.037958	46.400423
3382.614600	393902.007827	46.405428
3380.208823	384077.987996	46.410433
3377.362324	374205.976425	46.415437
3375.390616	364257.288866	46.420442
3373.258459	354252.962244	46.425447
3370.298044	344202.041664	46.430452
3367.884960	334106.887171	46.435457
3364.887401	323948.006309	46.440461
3362.255000	313739.215660	46.445466
3359.849590	303477.594392	46.450471
3356.577511	293171.233286	46.455476
3353.630642	282818.764958	46.460481
3350.693185	272429.951762	46.465485
3347.877069	261993.099982	46.470490
3344.941001	251530.478170	46.475495
3341.403565	240999.254038	46.480500
3338.443831	230421.197430	46.485505
3335.211622	219769.628567	46.490509
3331.771329	209166.004651	46.495514
3328.525402	198513.876396	46.500519
3324.927814	187852.312962	46.505524
3321.042882	177143.563488	46.510529
3317.236144	166452.111198	46.515533
3313.135980	155714.314096	46.520538
3309.539263	144978.604807	46.525543
3304.986915	134259.673673	46.530548
3300.808390	123512.234839	46.535553
3295.966699	112782.238992	46.540557
3290.857145	102063.556147	46.545562
3286.191249	91350.082698	46.550567
3280.687027	80674.549023	46.555572
3274.928951	70025.431642	46.560577
3267.920775	59434.808502	46.565581
3259.631017	48945.725326	46.570586
3248.466114	38616.914851	46.575591
3222.714366	28829.400385	46.580596
3185.847846	19576.524284	46.585601
3135.890481	11197.844643	46.590605
3072.585003	3940.849835	46.595610
2911.722216	422.988110	46.600615
2696.703707	380.039684	46.605620
2598.661865	375.280964	46.610625
2608.473459	384.898700	46.615629
2682.287295	372.168477	46.620634
2771.840811	350.896991	46.625639
2843.265032	348.465838	46.630644
2883.955251	330.086793	46.635649
2896.150166	337.183738	46.640653
2890.277179	341.811565	46.645658
2877.166581	353.270156	46.650663
2863.443606	362.071732	46.655668
2854.470596	345.261135	46.660673
2849.300483	336.192814	46.665677
2846.666248	332.619525	46.670682
2845.629634	340.156176	46.675687
2844.139249	342.019019	46.680692
2842.723799	324.219367	46.685697
2840.918555	325.777861	46.690701
2838.158752	327.684525	46.695706
2835.285107	318.818537	46.700711
2831.802553	332.086642	46.705716
2828.791706	325.524052	46.710721
2825.753104	318.057006	46.715725
2822.620128	326.847697	46.720730
2819.708042	308.872055	46.725735
2816.312572	306.708709	46.730740
2813.279372	314.897905	46.735745
2810.185493	329.536129	46.740749
2806.728451	323.020275	46.745754
2803.845647	308.450029	46.750759
2800.272789	322.382389	46.755764
2797.418757	311.281842	46.760769
2794.164661	305.743887	46.765773
2790.442551	321.250574	46.770778
2787.539564	303.539734	46.775783
2784.051697	309.445872	46.780788
2781.032888	296.762016	46.785793
2777.641730	298.515584	46.790797
2774.047745	311.755987	46.795802
2771.235922	300.112591	46.800807
2766.983254	308.739724	46.805812
2764.093601	297.986037	46.810817
2761.076491	296.027801	46.815821
2757.561099	297.131972	46.820826
2754.586993	298.017268	46.825831
2750.469380	308.048833	46.830836
2747.169887	297.515939	46.835841
2743.983267	301.556725	46.840845
2740.403853	291.239188	46.845850
2737.161636	280.526585	46.850855
2733.497706	296.702440	46.855860
2730.523769	292.539595	46.860865
2726.926083	292.275151	46.865869
2723.145410	286.022855	46.870874
2720.333562	286.260657	46.875879
2716.443944	294.358042	46.880884
2713.411335	282.456892	46.885889
2709.956249	288.602416	46.890893
2707.027207	285.935133	46.895898
2703.410678	278.541646	46.900903
2699.473100	291.838410	46.905908
2695.931041	285.894062	46.910913
2692.489428	284.435105	46.915917
2689.303567	281.724933	46.920922
2686.347728	280.064045	46.925927
2682.254906	279.250935	46.930932
2678.946592	280.621607	46.935937
2675.280120	280.915389	46.940941
2671.155462	277.755536	46.945946
2668.567181	274.615654	46.950951
2665.522963	272.208105	46.955956
2662.361453	269.298590	46.960961
2658.141325	277.052993	46.965965
2654.371574	277.401303	46.970970
2651.395307	269.225985	46.975975
2648.138352	267.560895	46.980980
2644.564411	275.192087	46.985985
2640.431366	267.902055	46.990989
2636.892943	279.681963	46.995994
2633.918844	272.689297	47.000999
2630.470356	271.985149	47.006004
2627.563880	260.329541	47.011009
2624.117424	261.018203	47.016013
2620.835047	269.057618	47.021018
2617.120037	263.325242	47.026023
2613.524829	271.620463	47.031028
2609.518479	255.520663	47.036033
2605.910984	261.647148	47.041037
2602.512692	268.609104	47.046042
2599.455853	264.215914	47.051047
2596.181420	265.564064	47.056052
2592.545899	258.993623	47.061057
2589.087365	270.021522	47.066061
2585.260747	267.787905	47.071066
2581.695356	266.355922	47.076071
2578.357739	270.739632	47.081076
2575.085155	264.888846	47.086081
2572.091995	271.053157	47.091085
2568.447129	279.257534	47.096090
2564.865199	274.985074	47.101095
2560.953319	264.527433	47.106100
2557.780226	260.475154	47.111105
2554.105293	268.198010	47.116109
2550.710756	272.895968	47.121114
2547.415969	250.417886	47.126119
2543.640661	266.638868	47.131124
2540.226996	265.014860	47.136129
2537.197531	258.276638	47.141133
2533.543827	267.346225	47.146138
2530.182514	254.765482	47.151143
2526.148730	258.740725	47.156148
2522.695850	249.816138	47.161153
2519.268254	255.685981	47.166157
2515.843801	263.128795	47.171162
2512.686559	262.381510	47.176167
2509.099342	261.390805	47.181172
2505.408085	252.477120	47.186177
2502.213376	257.296344	47.191181
2498.209034	266.352829	47.196186
2495.223164	246.283870	47.201191
2491.440104	256.772475	47.206196
2487.993345	260.682409	47.211201
2484.486767	254.833556	47.216205
2481.205985	254.456495	47.221210
2477.789880	243.807361	47.226215
2473.853996	244.081242	47.231220
2470.477160	244.632605	47.236225
2467.142955	249.884665	47.241229
2463.718246	252.250733	47.246234
2460.078762	242.240355	47.251239
2456.378364	247.652645	47.256244
2452.969165	261.656040	47.261249
2449.755486	244.942423	47.266253
2446.429275	249.652827	47.271258
2443.018485	244.379950	47.276263
2439.525119	242.379932	47.281268
2435.673653	241.530808	47.286273
2431.964504	246.422951	47.291277
2428.417871	250.421791	47.296282
2425.516534	240.453577	47.301287
2421.812953	240.046622	47.306292
2417.988504	241.907109	47.311297
2415.084979	242.950681	47.316301
2411.558376	232.227571	47.321306
2407.803346	238.984409	47.326311
2403.970424	243.336801	47.331316
2400.871329	243.500248	47.336321
2397.092163	242.840876	47.341325
2393.885069	245.296578	47.346330
2390.422656	237.949888	47.351335
2386.774677	243.678736	47.356340
2383.353517	242.224744	47.361345
2379.945461	240.933447	47.366349
2376.105946	242.849912	47.371354
2372.872072	235.152997	47.376359
2369.375601	240.391303	47.381364
2366.034343	241.614322	47.386369
2362.569727	238.138624	47.391373
2359.114608	237.214408	47.396378
2355.935574	236.681023	47.401383
2351.559429	244.698160	47.406388
2348.293962	232.062271	47.411393
2345.006006	233.502729	47.416397
2341.254464	243.619774	47.421402
2338.023485	231.957671	47.426407
2334.106707	237.248338	47.431412
2330.655040	229.375255	47.436417
2327.817238	228.663369	47.441421
2324.040572	237.202497	47.446426
2320.647369	228.148917	47.451431
2316.933239	233.079714	47.456436
2313.185885	234.456844	47.461441
2309.882483	226.062780	47.466445
2306.558844	246.637642	47.471450
2303.083596	236.478727	47.476455
2299.367275	235.296813	47.481460
2295.804547	240.010862	47.486465
2292.680786	227.457991	47.491469
2289.094910	235.944948	47.496474
2285.597554	235.649765	47.501479
2282.112433	235.371607	47.506484
2278.438691	242.673198	47.511489
2274.915327	236.590751	47.516493
2271.393977	234.518281	47.521498
2268.341275	231.074042	47.526503
2264.270743	237.269133	47.531508
2260.974632	226.499122	47.536513
2257.334897	232.517699	47.541517
2253.644355	232.498471	47.546522
2250.745464	223.882240	47.551527
2246.794452	238.630909	47.556532
2243.663026	236.098231	47.561537
2240.197331	236.378640	47.566541
2236.602819	228.064001	47.571546
2233.085744	233.472292	47.576551
2229.454188	235.445094	47.581556
2226.070505	224.918135	47.586561
2222.847991	225.936550	47.591565
2219.092422	235.159089	47.596570
2215.767596	227.506858	47.601575
2212.044886	230.451477	47.606580
2208.558680	224.500075	47.611585
2205.034083	219.202987	47.616589
2201.356135	226.179038	47.621594
2198.148422	217.229505	47.626599
2194.610987	226.177617	47.631604
2191.346796	218.340878	47.636609
2187.676028	221.723559	47.641613
2183.901901	225.340927	47.646618
2180.783352	213.466126	47.651623
2177.016408	228.012887	47.656628
2173.473836	216.870408	47.661633
2169.969994	219.233768	47.666637
2166.098748	219.740238	47.671642
2163.240239	204.257701	47.676647
2159.459935	220.043818	47.681652
2156.149870	216.510476	47.686657
2152.434190	209.953225	47.691661
2148.801926	219.008052	47.696666
2145.719168	221.136815	47.701671
2141.902742	222.501941	47.706676
2138.460891	210.985441	47.711681
2135.389596	217.805612	47.716685
2131.405855	212.621395	47.721690
2127.992214	210.141540	47.726695
2124.477762	218.385717	47.731700
2121.319108	216.412829	47.736705
2117.687608	216.409876	47.741709
2113.949173	220.861647	47.746714
2110.490674	209.796601	47.751719
2106.548617	222.570797	47.756724
2103.319955	225.874573	47.761729
2100.288879	212.623532	47.766733
2096.470454	217.171475	47.771738
2093.339687	215.998643	47.776743
2089.503141	214.413828	47.781748
2086.391094	211.135441	47.786753
2082.514476	214.362605	47.791757
2078.641202	209.894400	47.796762
2075.141854	210.651128	47.801767
2071.692810	232.646252	47.806772
2068.806804	229.693047	47.811777
2065.548203	213.933621	47.816781
2061.916894	216.218609	47.821786
2058.292328	212.355590	47.826791
2054.291323	210.885431	47.831796
2051.109889	214.667714	47.836801
2047.684493	213.794486	47.841805
2043.925476	215.703259	47.846810
2040.458551	206.563746	47.851815
2036.761059	209.498069	47.856820
2033.439543	214.653679	47.861825
2030.189832	205.728731	47.866829
2026.639790	214.223384	47.871834
2023.123168	216.846411	47.876839
2019.313609	211.206740	47.881844
2016.101379	202.494536	47.886849
2012.591071	211.415248	47.891853
2009.265739	211.811124	47.896858
2005.998577	207.053358	47.901863
2002.209229	216.266453	47.906868
1998.414183	205.776224	47.911873
1994.967402	206.283990	47.916877
1991.042579	213.945176	47.921882
1988.165081	199.674416	47.926887
1984.665455	211.234013	47.931892
1981.225640	208.079496	47.936897
1977.828274	207.907170	47.941901
1974.152442	210.219965	47.946906
1970.682884	198.440687	47.951911
1967.038068	206.785745	47.956916
1963.442509	210.431372	47.961921
1960.115863	203.404084	47.966925
1956.185693	200.728258	47.971930
1952.762108	200.289260	47.976935
1949.358292	206.298045	47.981940
1946.297250	207.518427	47.986945
1943.022044	209.785468	47.991949
1939.223526	201.102646	47.996954
1935.759091	193.767412	48.001959
1931.911114	211.284934	48.006964
1928.681655	204.070560	48.011969
1925.306529	198.930498	48.016973
1921.297739	210.109346	48.021978
1918.071776	206.260358	48.026983
1914.457659	197.170068	48.031988
1910.537332	199.872669	48.036993
1907.311572	198.508019	48.041997
1903.749882	201.105878	48.047002
1900.708568	200.905825	48.052007
1897.144843	213.627250	48.057012
1893.520603	207.326370	48.062017
1890.282884	200.337133	48.067021
1886.563939	203.072721	48.072026
1883.082681	208.102418	48.077031
1879.533824	206.868136	48.082036
1875.828103	197.568932	48.087041
1872.740291	204.848198	48.092045
1868.997414	204.073902	48.097050
1865.558856	199.711980	48.102055
1861.922738	209.643521	48.107060
1858.841386	196.522172	48.112065
1855.304708	204.618776	48.117069
1851.431031	198.914511	48.122074
1848.182972	203.461301	48.127079
1844.524881	199.353246	48.132084
1840.957476	198.110797	48.137089
1837.307626	196.785269	48.142093
1833.643535	196.048506	48.147098
1830.598957	191.995609	48.152103
1827.168743	199.698974	48.157108
1823.515924	194.736390	48.162113
1820.121979	189.816535	48.167117
1816.268354	189.040611	48.172122
1813.139874	194.928350	48.177127
1809.475911	204.981311	48.182132
1805.757519	189.324570	48.187137
1802.724856	193.675028	48.192141
1799.199449	206.268221	48.197146
1795.678729	191.221912	48.202151
1791.994156	190.438926	48.207156
1788.491339	188.814901	48.212161
1784.827100	198.232963	48.217165
1781.522640	190.545955	48.222170
1777.998456	187.055632	48.227175
1774.264216	189.389602	48.232180
1771.040997	190.946889	48.237185
1767.401235	180.232905	48.242189
1763.717472	190.730432	48.247194
1760.460674	190.904679	48.252199
1756.936343	184.077251	48.257204
1753.288624	184.753346	48.262209
1750.192970	191.681050	48.267213
1746.611277	199.210944	48.272218
1743.241134	178.907411	48.277223
1739.434477	179.120404	48.282228
1735.944837	181.277986	48.287233
1732.357999	184.755447	48.292237
1728.504606	183.511608	48.297242
1725.434956	189.449554	48.302247
1722.017470	184.600426	48.307252
1718.708648	186.515677	48.312257
1715.073736	182.950725	48.317261
1711.419286	187.652426	48.322266
1708.021629	178.485019	48.327271
1704.345005	188.449733	48.332276
1700.616267	181.071332	48.337281
1696.941519	179.258484	48.342285
1693.593340	179.375230	48.347290
1690.596872	182.519901	48.352295
1687.144983	180.742895	48.357300
1683.291994	183.000709	48.362305
1680.121320	180.521933	48.367309
1676.276666	178.726280	48.372314
1672.906737	184.978980	48.377319
1669.360233	189.742701	48.382324
1665.908043	180.557777	48.387329
1662.719915	179.264380	48.392333
1659.060491	188.586589	48.397338
1655.681317	180.423044	48.402343
1651.755079	180.107486	48.407348
1648.249032	180.621742	48.412353
1644.945940	182.874075	48.417357
1641.393858	185.309856	48.422362
1637.811635	188.201373	48.427367
1634.121249	185.234002	48.432372
1630.837632	179.116514	48.437377
1627.530145	187.193140	48.442381
1623.810461	186.279594	48.447386
1620.528122	179.012560	48.452391
1616.681708	187.833591	48.457396
1613.370432	190.404073	48.462401
1609.778778	188.031103	48.467405
1606.438248	176.015801	48.472410
1603.181003	165.216413	48.477415
1599.204455	178.719619	48.482420
1595.728396	178.296359	48.487425
1592.314577	178.493340	48.492429
1588.352507	181.890624	48.497434
1585.392642	188.078553	48.502439
1581.905192	185.534104	48.507444
1578.469373	177.723669	48.512449
1574.963932	176.490864	48.517453
1570.981739	178.954446	48.522458
1567.736802	168.734620	48.527463
1564.241082	177.519699	48.532468
1560.960864	181.749993	48.537473
1557.361933	172.011625	48.542477
1553.424401	188.388379	48.547482
1550.539081	185.536021	48.552487
1546.960566	178.477627	48.557492
1543.405844	176.597206	48.562497
1539.548743	180.935733	48.567501
1536.226829	179.435689	48.572506
1532.784768	171.165098	48.577511
1528.985147	183.242469	48.582516
1525.363905	184.728121	48.587521
1522.858654	177.115361	48.592525
1519.151863	183.166027	48.597530
1515.619751	176.672494	48.602535
1511.968746	179.441149	48.607540
1508.380529	178.078100	48.612545
1504.702206	175.319245	48.617549
1500.800414	175.340494	48.622554
1497.674331	172.704588	48.627559
1494.333891	180.686071	48.632564
1490.672816	160.226338	48.637569
1487.367794	167.735725	48.642573
1483.588443	179.072809	48.647578
1480.414468	168.889565	48.652583
1476.958533	175.628800	48.657588
1473.309585	179.117814	48.662593
1469.848218	167.938822	48.667597
1466.326128	169.839856	48.672602
1462.799837	172.610544	48.677607
1459.156438	172.757477	48.682612
1455.258404	169.455705	48.687617
1452.087525	171.493528	48.692621
1448.691495	172.459227	48.697626
1445.233229	171.880979	48.702631
1441.747409	167.380194	48.707636
1438.186807	172.859228	48.712641
1434.870937	171.138334	48.717645
1431.436922	179.904896	48.722650
1428.056267	172.747327	48.727655
1424.337133	169.853781	48.732660
1420.247800	171.013239	48.737665
1417.226051	170.487168	48.742669
1413.899955	170.621908	48.747674
1410.496216	153.454529	48.752679
1406.706355	170.008697	48.757684
1402.938443	163.537875	48.762689
1399.274026	166.701644	48.767693
1396.107265	169.222717	48.772698
1393.085005	167.584596	48.777703
1389.208375	169.538264	48.782708
1385.436748	168.605305	48.787713
1382.255382	167.884506	48.792717
1378.587138	177.845301	48.797722
1375.151651	160.936722	48.802727
1371.464762	167.305486	48.807732
1368.015187	168.846641	48.812737
1364.448691	172.125576	48.817741
1360.852842	172.540751	48.822746
1358.164057	164.873223	48.827751
1354.537615	166.848557	48.832756
1350.577993	177.926586	48.837761
1347.656671	164.932753	48.842765
1343.633811	166.949944	48.847770
1339.839735	163.057204	48.852775
1336.326066	168.602132	48.857780
1332.873110	161.344483	48.862785
1329.642767	160.695919	48.867789
1325.965328	164.704292	48.872794
1322.669679	167.360913	48.877799
1319.222435	169.804207	48.882804
1315.606503	162.920932	48.887809
1312.527753	153.534898	48.892813
1308.769195	164.864371	48.897818
1305.610677	167.730600	48.902823
1301.276596	154.999391	48.907828
1297.900680	165.941134	48.912833
1294.846585	166.842672	48.917837
1290.990167	175.309843	48.922842
1287.829682	162.304912	48.927847
1284.098333	154.364085	48.932852
1280.551779	168.227662	48.937857
1276.835393	162.560839	48.942861
1273.440102	160.560623	48.947866
1269.788155	165.200058	48.952871
1266.422034	172.419016	48.957876
1263.419920	166.053908	48.962881
1259.694874	165.353260	48.967885
1255.944329	166.936749	48.972890
1252.479224	157.244562	48.977895
1249.216991	177.479646	48.982900
1245.561672	169.942511	48.987905
1242.112219	164.290149	48.992909
1238.639633	169.478310	48.997914
1235.101661	160.988240	49.002919
1231.176356	160.429581	49.007924
1227.695954	160.233933	49.012929
1224.882096	163.474623	49.017933
1220.998217	162.864046	49.022938
1217.549457	160.016553	49.027943
1214.156887	163.479056	49.032948
1210.255588	163.137039	49.037953
1207.015418	157.458932	49.042957
1203.145108	167.457393	49.047962
1200.079652	161.055717	49.052967
1197.126126	162.347353	49.057972
1193.060997	167.203014	49.062977
1189.704666	154.685082	49.067981
1185.769197	163.550397	49.072986
1182.547389	163.070774	49.077991
1178.948272	156.209373	49.082996
1175.076493	158.729129	49.088001
1172.096623	163.709900	49.093005
1168.379764	175.364432	49.098010
1164.980309	156.313967	49.103015
1161.152161	160.126212	49.108020
1158.100680	167.192742	49.113025
1154.758359	160.833046	49.118029
1150.425854	174.017055	49.123034
1147.316885	160.738322	49.128039
1143.987375	165.685173	49.133044
1140.677757	165.444012	49.138049
1137.277380	166.291107	49.143053
1133.584320	162.691295	49.148058
1129.899720	162.396617	49.153063
1126.389107	165.913177	49.158068
1122.649454	156.750397	49.163073
1119.359715	154.098681	49.168077
1115.734150	166.315586	49.173082
1112.543215	157.972220	49.178087
1108.946891	155.292593	49.183092
1105.311837	164.914464	49.188097
1102.201917	158.049199	49.193101
1098.130403	162.417030	49.198106
1094.712910	165.411933	49.203111
1091.211142	160.355392	49.208116
1087.791992	163.004884	49.213121
1085.174373	173.515197	49.218125
1080.819271	169.607696	49.223130
1077.520445	151.815804	49.228135
1073.813457	163.797062	49.233140
1070.439860	162.668933	49.238145
1067.087601	155.845178	49.243149
1063.425641	163.135748	49.248154
1059.985076	162.775169	49.253159
1056.158235	163.434827	49.258164
1052.655961	154.986234	49.263169
1049.372341	160.862772	49.268173
1045.694796	170.045370	49.273178
1042.619142	161.166254	49.278183
1038.831247	164.006676	49.283188
1035.222530	172.550470	49.288193
1031.970090	148.955850	49.293197
1027.964976	158.944184	49.298202
1024.925883	151.653215	49.303207
1021.569688	156.435822	49.308212
1017.957667	158.377178	49.313217
1014.666921	153.107080	49.318221
1010.687481	154.368794	49.323226
1007.276271	148.457897	49.328231
1003.741753	151.980729	49.333236
1000.024562	169.849665	49.338241
997.023835	149.124825	49.343245
993.344907	160.353478	49.348250
989.673563	161.092173	49.353255
986.514744	157.114589	49.358260
982.875561	158.931506	49.363265
979.201943	158.218576	49.368269
975.646148	159.219860	49.373274
972.203181	150.366906	49.378279
968.886685	153.008284	49.383284
965.462478	162.624800	49.388289
962.113230	146.769827	49.393293
958.256505	165.684371	49.398298
954.783593	168.961667	49.403303
951.478076	160.364627	49.408308
947.648178	165.822741	49.413313
944.297850	158.463827	49.418317
940.409209	158.982121	49.423322
937.281016	154.610806	49.428327
933.701683	157.838991	49.433332
930.009254	161.458867	49.438337
926.778049	158.123868	49.443341
923.017206	161.969027	49.448346
920.015455	155.466316	49.453351
916.498484	159.223559	49.458356
912.617741	164.528589	49.463361
909.320593	158.427250	49.468365
905.785818	157.665390	49.473370
902.747995	152.031976	49.478375
898.945209	150.385834	49.483380
895.100909	160.989431	49.488385
891.417861	151.215860	49.493389
887.907679	151.974465	49.498394
884.703208	157.017587	49.503399
881.341607	152.804412	49.508404
877.392278	155.232659	49.513409
874.496065	157.646145	49.518413
870.872303	160.551697	49.523418
867.400518	152.108050	49.528423
863.712993	165.737272	49.533428
860.224924	163.705927	49.538433
856.791927	152.552044	49.543437
853.003592	164.725492	49.548442
849.553805	152.559819	49.553447
846.259051	153.773680	49.558452
842.343606	160.986245	49.563457
839.150266	156.682464	49.568461
835.371203	156.585467	49.573466
832.509746	145.610007	49.578471
828.661601	143.028159	49.583476
824.992185	151.323879	49.588481
822.108545	143.217521	49.593485
818.312038	161.994608	49.598490
814.253081	155.840952	49.603495
811.200662	151.587019	49.608500
807.297527	150.321637	49.613505
803.934162	153.909336	49.618509
800.735462	145.132467	49.623514
797.080744	150.185160	49.628519
794.021548	156.490395	49.633524
790.459039	154.682405	49.638529
786.740560	154.539323	49.643533
782.739025	156.103051	49.648538
779.658633	148.495051	49.653543
775.863268	156.487219	49.658548
772.367533	158.111364	49.663553
769.136256	146.258014	49.668557
765.303034	157.686862	49.673562
762.345391	155.297663	49.678567
758.793865	155.644766	49.683572
755.118945	155.701191	49.688577
751.756514	152.320870	49.693581
748.247778	153.659595	49.698586
744.624612	148.519619	49.703591
741.083219	143.046403	49.708596
737.658260	141.221845	49.713601
734.035211	141.053366	49.718605
730.128429	152.244976	49.723610
727.005487	146.780303	49.728615
723.414924	141.382895	49.733620
719.786507	149.632233	49.738625
716.434802	141.460773	49.743629
712.935270	142.123000	49.748634
709.873277	151.031140	49.753639
706.504323	154.677027	49.758644
702.678010	148.555666	49.763649
699.464637	138.649614	49.768653
695.532065	155.416036	49.773658
692.072989	148.695674	49.778663
688.133786	156.501603	49.783668
684.813487	155.745975	49.788673
681.189879	148.128989	49.793677
677.610981	155.848880	49.798682
674.700056	153.602554	49.803687
671.189075	155.543977	49.808692
667.370896	146.934210	49.813697
664.310317	153.140675	49.818701
660.289652	151.974702	49.823706
656.966059	147.384729	49.828711
653.549730	151.826025	49.833716
649.584252	152.939042	49.838721
646.571027	148.195707	49.843725
643.051912	146.951844	49.848730
639.705994	153.421301	49.853735
636.468980	147.076180	49.858740
632.346054	151.814527	49.863745
629.189413	143.583376	49.868749
625.444683	155.829724	49.873754
621.810695	144.149033	49.878759
618.376651	150.002551	49.883764
614.925417	147.833457	49.888769
611.252785	140.174993	49.893773
607.823681	139.980766	49.898778
604.515584	137.968477	49.903783
601.165722	142.386189	49.908788
597.424209	146.818770	49.913793
594.039397	140.077029	49.918797
590.654050	141.464810	49.923802
586.785725	142.697665	49.928807
583.453850	147.484738	49.933812
579.920019	136.624129	49.938817
576.422240	137.969321	49.943821
572.937044	148.901756	49.948826
569.523035	139.327449	49.953831
565.908710	145.330335	49.958836
562.326947	147.495513	49.963841
558.776964	134.656999	49.968845
555.255942	142.353963	49.973850
551.813178	143.679229	49.978855
548.998417	148.524448	49.983860
545.360133	139.678275	49.988865
541.554722	138.031103	49.993869
537.612895	145.490373	49.998874
534.150697	137.825022	50.003879
530.740944	144.123050	50.008884
527.450264	144.395524	50.013889
524.002918	139.867602	50.018893
520.179436	145.145321	50.023898
517.126484	148.674087	50.028903
513.317712	142.954733	50.033908
509.464405	145.680261	50.038913
506.044650	145.578955	50.043917
502.553307	147.438593	50.048922
499.442300	137.117189	50.053927
496.080184	152.423692	50.058932
492.511643	149.557612	50.063937
489.075987	141.194066	50.068941
485.357484	141.982951	50.073946
481.873423	137.446123	50.078951
478.279617	143.488676	50.083956
474.794559	141.159607	50.088961
471.724906	143.150069	50.093965
467.699680	145.372567	50.098970
464.362168	136.348811	50.103975
460.771140	138.572298	50.108980
456.716180	144.078887	50.113985
453.816545	148.912118	50.118989
450.388669	137.295663	50.123994
447.035142	136.376456	50.128999
443.060977	137.263534	50.134004
439.834747	147.533104	50.139009
436.449484	135.073327	50.144013
432.617375	142.079658	50.149018
429.314843	140.694773	50.154023
425.733655	135.199714	50.159028
422.127715	151.134202	50.164033
419.082941	144.403280	50.169037
415.358335	137.486433	50.174042
411.782831	136.635483	50.179047
408.007604	140.640639	50.184052
404.440808	139.324086	50.189057
401.274648	137.534304	50.194061
397.571741	149.271985	50.199066
394.251618	140.627880	50.204071
391.339859	137.856592	50.209076
387.322922	150.536707	50.214081
383.598225	143.834368	50.219085
379.706486	142.995228	50.224090
376.634346	145.700797	50.229095
373.172902	145.295786	50.234100
369.627896	151.459965	50.239105
366.557970	134.742802	50.244109
362.737341	144.160850	50.249114
359.271003	147.748801	50.254119
355.678977	139.249576	50.259124
352.208251	141.372153	50.264129
348.603013	140.302106	50.269133
344.929910	146.229476	50.274138
341.620059	142.456834	50.279143
338.246840	145.261092	50.284148
334.516830	149.977122	50.289153
331.153227	141.784182	50.294157
327.456722	144.494267	50.299162
324.260470	145.597303	50.304167
320.831662	148.102458	50.309172
317.209686	145.682249	50.314177
313.998240	144.472286	50.319181
310.625423	144.923587	50.324186
306.607980	142.635509	50.329191
302.845439	141.152662	50.334196
298.946434	143.034571	50.339201
296.080157	139.440734	50.344205
293.068488	139.406587	50.349210
289.077262	141.569314	50.354215
285.408706	136.764260	50.359220
282.054146	132.658190	50.364225
278.697937	132.592381	50.369229
275.031437	141.818084	50.374234
271.608720	137.860803	50.379239
268.430898	137.105826	50.384244
264.570584	137.580375	50.389249
261.411850	134.356980	50.394253
257.585368	143.043145	50.399258
254.092483	133.227249	50.404263
250.634758	139.243681	50.409268
246.663297	145.607908	50.414273
243.584640	131.046486	50.419277
240.216438	137.322784	50.424282
236.556865	137.935940	50.429287
233.574245	133.083589	50.434292
229.687960	139.841784	50.439297
226.385731	135.405388	50.444301
222.679428	141.165561	50.449306
218.957725	131.167496	50.454311
215.192655	139.304290	50.459316
211.831305	144.684877	50.464321
208.791526	131.542309	50.469325
205.096666	137.344500	50.474330
201.718624	136.468344	50.479335
198.026659	137.315061	50.484340
194.367329	140.043739	50.489345
190.667657	137.924909	50.494349
187.026788	141.245031	50.499354
183.905248	132.318061	50.504359
180.696532	145.469581	50.509364
177.151364	152.281249	50.514369
173.896400	137.289268	50.519373
170.433088	139.657251	50.524378
166.564239	129.524605	50.529383
162.918499	134.280959	50.534388
159.253546	138.026130	50.539393
156.066322	125.072125	50.544397
152.754681	133.849071	50.549402
149.218711	137.519563	50.554407
145.539027	140.512965	50.559412
141.616603	127.938723	50.564417
138.613878	122.300121	50.569421
134.956174	136.968455	50.574426
131.466022	131.124395	50.579431
128.221171	129.007796	50.584436
124.567043	140.033539	50.589441
120.977277	134.278455	50.594445
117.460552	143.857626	50.599450
113.752838	129.091940	50.604455
110.386363	125.260619	50.609460
106.871893	140.549905	50.614465
103.666813	130.223569	50.619469
100.115383	133.267623	50.624474
96.801428	131.035787	50.629479
93.161890	126.090808	50.634484
89.485825	128.627762	50.639489
85.770830	135.414060	50.644493
81.932603	135.207711	50.649498
78.812354	125.798374	50.654503
75.431611	131.197615	50.659508
71.704366	131.580049	50.664513
68.518257	127.574714	50.669517
64.973809	141.137003	50.674522
61.496428	139.063007	50.679527
58.010958	135.601598	50.684532
54.544955	141.928181	50.689537
51.063829	138.974815	50.694541
47.019273	133.109364	50.699546
43.557387	135.934438	50.704551
40.670274	134.418763	50.709556
37.033849	134.729089	50.714561
33.390401	135.085564	50.719565
29.590657	139.273542	50.724570
26.703258	136.951919	50.729575
23.218798	127.124724	50.734580
19.142761	134.632194	50.739585
15.814432	140.581481	50.744589
12.204323	146.744359	50.749594
8.793214	132.214942	50.754599
5.729384	136.387372	50.759604
1.873676	136.151405	50.764609