Mon Mar 08 17:46:42 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
1.239994	91.706794	0.000000
1.000941	67.850584	0.005005
0.255239	31.844582	0.010010
-3.006994	8.074810	0.015014
-7.055564	5.595920	0.020019
-12.426508	11.537394	0.025024
-16.956923	13.894520	0.030029
-21.054008	6.995393	0.035034
-25.061106	17.420179	0.040038
-28.582403	4.067929	0.045043
-32.603980	19.591647	0.050048
-35.962330	8.878414	0.055053
-39.742281	-3.751327	0.060058
-43.575107	11.111526	0.065062
-47.223857	-4.787586	0.070067
-51.299335	12.250708	0.075072
-55.030252	2.104704	0.080077
-58.333665	4.770805	0.085082
-62.370434	7.869272	0.090086
-65.594811	-4.606197	0.095091
-69.696005	14.211840	0.100096
-73.561998	7.011022	0.105101
-77.284260	1.897205	0.110106
-81.321793	3.357404	0.115110
-84.809240	-0.078168	0.120115
-88.978721	1.622283	0.125120
-92.421383	1.817533	0.130125
-96.221659	7.732554	0.135130
-100.274184	8.252178	0.140134
-103.450331	3.879166	0.145139
-107.616178	5.883415	0.150144
-111.000409	4.177066	0.155149
-114.524148	10.306615	0.160154
-118.851973	10.430227	0.165158
-122.675624	13.666678	0.170163
-126.594367	10.249510	0.175168
-129.986366	1.430942	0.180173
-133.875240	0.935785	0.185178
-137.523477	6.487574	0.190182
-141.437267	3.604218	0.195187
-145.258727	11.883342	0.200192
-148.577030	9.896873	0.205197
-152.451266	-0.899448	0.210202
-156.575010	2.235124	0.215206
-160.206310	-3.421339	0.220211
-164.177129	3.866104	0.225216
-167.758343	-0.090538	0.230221
-171.273239	2.317726	0.235226
-175.179778	13.284924	0.240230
-178.618527	3.636542	0.245235
-182.598516	4.818074	0.250240
-186.282112	2.243407	0.255245
-190.356363	1.905650	0.260250
-194.312915	8.585329	0.265254
-197.986717	5.160735	0.270259
-202.352278	10.254657	0.275264
-205.565218	6.546806	0.280269
-209.219027	0.283742	0.285274
-213.094559	11.354854	0.290278
-216.598668	2.951688	0.295283
-220.002224	1.713767	0.300288
-224.113539	-0.936087	0.305293
-228.020997	2.788550	0.310298
-231.370211	3.025853	0.315302
-235.218698	1.086266	0.320307
-239.271875	6.688630	0.325312
-242.829725	-6.245859	0.330317
-246.585150	-0.363003	0.335322
-250.448297	3.435021	0.340326
-254.076038	-2.415825	0.345331
-257.874487	-0.711222	0.350336
-261.993099	0.932520	0.355341
-265.496015	-1.148898	0.360346
-269.564929	7.669783	0.365350
-273.084772	-0.317631	0.370355
-276.845710	6.665263	0.375360
-280.385773	3.881759	0.380365
-284.027898	-0.960672	0.385370
-288.089097	5.625469	0.390374
-291.774924	3.611128	0.395379
-295.526289	6.711731	0.400384
-299.512444	6.733826	0.405389
-302.910409	2.768642	0.410394
-306.914567	-0.216709	0.415398
-310.702847	-1.774708	0.420403
-314.577052	3.291444	0.425408
-318.326586	4.619335	0.430413
-321.841729	3.769945	0.435418
-325.786773	7.652121	0.440422
-329.310421	2.849194	0.445427
-332.800483	10.996854	0.450432
-336.619935	6.372037	0.455437
-340.811778	1.507056	0.460442
-344.923687	10.460451	0.465446
-348.085463	-4.180239	0.470451
-351.986764	11.793090	0.475456
-355.610817	8.340299	0.480461
-359.539334	8.335947	0.485466
-363.757065	10.757336	0.490470
-366.896202	1.701644	0.495475
-370.756546	3.009460	0.500480
-374.511286	6.120183	0.505485
-378.324952	5.618145	0.510490
-382.403593	6.377369	0.515494
-385.656965	0.902193	0.520499
-389.681809	8.655920	0.525504
-393.415751	4.350275	0.530509
-396.909502	-6.228826	0.535514
-401.144265	3.037575	0.540518
-404.711810	-9.265913	0.545523
-408.759650	1.178572	0.550528
-412.298312	-1.928224	0.555533
-415.756325	-5.897846	0.560538
-419.958846	-1.704763	0.565542
-423.271781	-13.419678	0.570547
-427.108550	1.236185	0.575552
-430.952337	4.665556	0.580557
-434.874415	-0.395286	0.585562
-438.781885	4.411448	0.590566
-442.404968	-6.605812	0.595571
-446.150874	-1.484251	0.600576
-450.167916	-7.588010	0.605581
-453.500824	-11.112361	0.610586
-457.422540	0.228248	0.615590
-460.715453	-9.767822	0.620595
-464.767827	5.313600	0.625600
-468.676394	-7.644943	0.630605
-472.335542	1.775661	0.635610
-476.544298	4.752460	0.640614
-479.833290	-6.770661	0.645619
-483.558833	0.957496	0.650624
-487.709969	-6.960312	0.655629
-491.346550	-2.773903	0.660634
-495.066815	3.579939	0.665638
-498.605756	-2.847660	0.670643
-502.557234	-6.721006	0.675648
-506.384807	-1.203123	0.680653
-509.898822	-8.227601	0.685658
-514.154532	-3.188524	0.690662
-517.705389	-7.887470	0.695667
-521.239418	-4.909539	0.700672
-524.704338	1.133916	0.705677
-528.858437	-7.614377	0.710682
-532.592645	4.387090	0.715686
-536.309563	-12.088488	0.720691
-540.475728	-0.762331	0.725696
-544.258477	-2.748184	0.730701
-547.787500	-6.248964	0.735706
-551.644618	2.056957	0.740710
-555.157132	-5.361921	0.745715
-558.665222	-8.333032	0.750720
-562.586887	-1.995810	0.755725
-566.297419	-10.931567	0.760730
-570.418316	-1.918034	0.765734
-574.173434	-6.529077	0.770739
-577.813143	-6.120318	0.775744
-581.942422	-0.960972	0.780749
-585.196558	-2.515542	0.785754
-589.196620	0.368196	0.790758
-592.792931	-11.766390	0.795763
-596.755895	-2.391698	0.800768
-600.372139	-3.558832	0.805773
-603.798417	-6.377368	0.810778
-607.885688	2.405359	0.815782
-611.590054	-7.769185	0.820787
-615.613536	2.515622	0.825792
-619.330081	-4.752296	0.830797
-623.037221	-4.108776	0.835802
-626.741661	1.160972	0.840806
-630.282834	-9.810717	0.845811
-634.312228	2.990234	0.850816
-638.329737	1.641259	0.855821
-641.697332	-0.568448	0.860826
-645.470698	2.425820	0.865830
-649.369925	-17.540093	0.870835
-652.874629	2.713110	0.875840
-656.746445	2.649727	0.880845
-660.562861	-1.760578	0.885850
-664.609639	-3.935863	0.890854
-668.147104	-6.714465	0.895859
-672.205833	5.917774	0.900864
-675.847732	-2.005358	0.905869
-679.194643	2.593932	0.910874
-682.923535	3.405019	0.915878
-686.539572	4.399926	0.920883
-690.386232	9.299843	0.925888
-694.642768	-0.970846	0.930893
-698.643016	2.499712	0.935898
-702.379287	0.697493	0.940902
-705.775629	1.860749	0.945907
-709.476490	6.565517	0.950912
-713.256338	1.659037	0.955917
-716.953123	-8.030854	0.960922
-721.006079	0.648804	0.965926
-724.518865	-7.840486	0.970931
-728.045819	-8.149661	0.975936
-731.896342	-11.370138	0.980941
-735.679810	-12.224923	0.985946
-739.892027	5.449664	0.990950
-743.485548	-5.682210	0.995955
-747.317596	-6.885596	1.000960
-750.842385	-8.294187	1.005965
-754.695243	-0.827554	1.010970
-758.638768	-3.528516	1.015974
-762.120467	-7.489105	1.020979
-765.901090	0.916879	1.025984
-769.810352	1.761655	1.030989
-773.694191	-8.875931	1.035994
-777.374677	-2.753526	1.040998
-780.958054	0.428205	1.046003
-784.938490	-8.580749	1.051008
-788.325252	0.937121	1.056013
-791.858480	-6.708304	1.061018
-796.261217	2.215027	1.066022
-799.710233	-11.868160	1.071027
-803.627870	-5.297821	1.076032
-807.638745	-2.497148	1.081037
-811.318071	-6.404002	1.086042
-814.968120	8.947965	1.091046
-818.393449	-4.864603	1.096051
-822.444487	0.927597	1.101056
-826.328464	3.927211	1.106061
-829.852659	-6.037652	1.111066
-834.184308	2.101701	1.116070
-837.512977	-14.626207	1.121075
-841.274061	-8.024063	1.126080
-844.969429	0.437797	1.131085
-848.564942	-4.378076	1.136090
-852.627654	-5.055582	1.141094
-856.146021	-5.660820	1.146099
-860.138514	3.523472	1.151104
-864.168305	2.320344	1.156109
-867.534021	1.451033	1.161114
-871.370163	6.032595	1.166118
-874.680495	-2.840472	1.171123
-878.417007	-0.085114	1.176128
-882.726907	-0.426597	1.181133
-886.247316	-7.645003	1.186138
-890.544557	4.945282	1.191142
-893.988676	-2.898727	1.196147
-897.656551	11.358679	1.201152
-901.475075	10.142343	1.206157
-904.871434	1.114342	1.211162
-908.854891	1.375138	1.216166
-912.759922	4.933327	1.221171
-916.644394	3.129912	1.226176
-920.479614	6.134498	1.231181
-923.817717	2.277348	1.236186
-928.144884	2.403896	1.241190
-931.406980	-1.708236	1.246195
-935.439560	-8.647571	1.251200
-939.252537	7.847061	1.256205
-942.780513	-5.018522	1.261210
-946.548348	1.927054	1.266214
-950.148117	-6.682010	1.271219
-954.016555	3.097589	1.276224
-958.027071	6.485065	1.281229
-961.418274	-6.824963	1.286234
-965.452354	-3.941472	1.291238
-968.744413	-5.066834	1.296243
-972.823226	-7.174962	1.301248
-976.959776	-2.037441	1.306253
-980.204417	-5.087883	1.311258
-984.352172	-2.104185	1.316262
-987.893867	-11.761649	1.321267
-991.665073	-6.195259	1.326272
-995.528587	-4.382899	1.331277
-999.309681	-4.201615	1.336282
-1003.337457	-4.155916	1.341286
-1006.519807	-11.607954	1.346291
-1010.122843	-5.354089	1.351296
-1014.224126	-1.841623	1.356301
-1018.182820	-8.275400	1.361306
-1022.224672	-6.696246	1.366310
-1025.567718	-5.064833	1.371315
-1029.172899	-3.262191	1.376320
-1033.273976	-5.210539	1.381325
-1036.645129	-8.054595	1.386330
-1040.945795	-4.440816	1.391334
-1044.612085	-6.822938	1.396339
-1048.280853	-6.508155	1.401344
-1051.951882	-5.038713	1.406349
-1055.513851	-9.097977	1.411354
-1059.504899	-4.726307	1.416358
-1063.006890	-5.559350	1.421363
-1066.899073	-0.828175	1.426368
-1070.665588	4.876359	1.431373
-1074.502314	-8.297583	1.436378
-1078.316203	-9.621597	1.441382
-1082.229510	-9.911027	1.446387
-1085.981282	0.941330	1.451392
-1089.662449	4.831421	1.456397
-1093.105816	-1.971644	1.461402
-1097.165942	0.515703	1.466406
-1100.877659	-6.031545	1.471411
-1104.541730	-7.901433	1.476416
-1108.600279	-1.155110	1.481421
-1112.269368	-3.601330	1.486426
-1116.104403	5.728492	1.491430
-1119.482972	2.888895	1.496435
-1123.434226	-2.472019	1.501440
-1127.187460	-4.578337	1.506445
-1130.671216	-4.609976	1.511450
-1134.901686	9.515408	1.516454
-1138.706001	-1.090106	1.521459
-1141.757428	0.341865	1.526464
-1145.678723	0.556850	1.531469
-1149.374363	-0.174127	1.536474
-1153.666548	11.056511	1.541478
-1157.273584	-3.084402	1.546483
-1160.997136	-1.161703	1.551488
-1165.153916	0.215315	1.556493
-1168.692213	2.896842	1.561498
-1172.549070	4.104473	1.566502
-1175.723629	-7.415395	1.571507
-1180.020250	-2.693453	1.576512
-1183.629340	3.250990	1.581517
-1187.229908	-3.558317	1.586522
-1191.363054	-1.382392	1.591526
-1195.060959	3.369948	1.596531
-1198.299675	-2.532168	1.601536
-1202.381488	-0.936851	1.606541
-1205.668123	-3.284842	1.611546
-1209.900181	4.925967	1.616550
-1213.544858	-9.317627	1.621555
-1217.368758	-4.854169	1.626560
-1221.544077	-4.164768	1.631565
-1225.041025	-4.544227	1.636570
-1228.776030	1.984958	1.641574
-1232.165368	-1.805195	1.646579
-1236.257731	-3.220008	1.651584
-1240.019298	-0.933145	1.656589
-1243.512757	-7.027815	1.661594
-1247.787176	4.077138	1.666598
-1251.385104	-6.349893	1.671603
-1255.169012	3.727295	1.676608
-1259.140285	-1.262761	1.681613
-1262.237534	-1.327664	1.686618
-1266.192685	4.859927	1.691622
-1270.161125	2.190632	1.696627
-1273.958318	-9.292534	1.701632
-1277.926655	7.711554	1.706637
-1281.433424	-2.132372	1.711642
-1285.163830	-2.439690	1.716646
-1288.771728	0.235807	1.721651
-1292.727243	8.252703	1.726656
-1296.447672	7.929613	1.731661
-1300.068782	1.945338	1.736666
-1303.933587	0.697649	1.741670
-1307.696174	8.847692	1.746675
-1311.322960	2.238315	1.751680
-1315.712122	2.336078	1.756685
-1318.714675	5.562852	1.761690
-1322.814620	6.587289	1.766694
-1326.717348	-1.753487	1.771699
-1330.399709	1.339254	1.776704
-1334.005996	2.349359	1.781709
-1337.570230	2.993206	1.786714
-1341.931981	10.359286	1.791718
-1345.389716	6.736360	1.796723
-1348.831553	-2.602203	1.801728
-1352.735737	-3.848237	1.806733
-1356.495360	-5.237246	1.811738
-1360.616155	2.546021	1.816742
-1364.154221	-1.281628	1.821747
-1367.746771	1.058808	1.826752
-1371.790765	6.024504	1.831757
-1375.145767	2.292145	1.836762
-1379.245404	-2.822226	1.841766
-1383.025593	5.091059	1.846771
-1386.571043	1.275665	1.851776
-1390.776832	-6.407803	1.856781
-1394.072395	-11.963074	1.861786
-1397.902500	-4.254661	1.866790
-1401.708365	-8.801024	1.871795
-1405.640100	-0.994330	1.876800
-1409.590538	3.762495	1.881805
-1413.053794	-6.845089	1.886810
-1416.613696	2.829068	1.891814
-1420.489404	-6.744265	1.896819
-1424.040988	-5.706510	1.901824
-1428.245482	4.797802	1.906829
-1431.611136	-1.112038	1.911834
-1435.702273	0.735905	1.916838
-1439.025680	-3.310487	1.921843
-1443.123609	-4.154781	1.926848
-1447.026769	4.847425	1.931853
-1450.784464	-6.042534	1.936858
-1454.581327	-2.332049	1.941862
-1458.236009	-2.632289	1.946867
-1461.628495	-9.135426	1.951872
-1465.563855	-1.444746	1.956877
-1469.122208	-2.750680	1.961882
-1473.239146	-1.194998	1.966886
-1477.011889	-1.424268	1.971891
-1480.581005	-7.769793	1.976896
-1485.079116	-0.985578	1.981901
-1488.302356	-4.281563	1.986906
-1491.969628	-4.622309	1.991910
-1496.010761	-1.470291	1.996915
-1499.664744	-1.656447	2.006912
-1500.488561	-3.640099	2.016909
-1498.152596	-5.460215	2.026906
-1495.212770	-3.466046	2.036902
-1493.142474	2.450426	2.046899
-1491.467144	-1.981220	2.056896
-1489.588801	-4.084892	2.066893
-1487.529864	-5.118554	2.076890
-1485.612510	-1.827006	2.086886
-1483.722470	1.576284	2.096883
-1481.715963	-0.080544	2.106880
-1479.769141	-4.836695	2.116877
-1478.057467	-2.072724	2.126874
-1476.272446	-4.665118	2.136870
-1474.192782	-8.809387	2.146867
-1472.243332	-1.564630	2.156864
-1470.415413	5.116970	2.166861
-1468.437196	2.899431	2.176858
-1466.465995	8.929690	2.186854
-1464.576331	4.844264	2.196851
-1462.813704	6.093807	2.206848
-1460.903700	4.095611	2.216845
-1459.391142	9.927731	2.226842
-1457.082416	5.595224	2.236838
-1455.278654	5.462952	2.246835
-1453.527881	5.427584	2.256832
-1451.162456	6.528527	2.266829
-1449.578346	6.246691	2.276826
-1447.739905	3.581030	2.286822
-1445.883094	10.810649	2.296819
-1444.043692	7.988523	2.306816
-1442.059071	1.579541	2.316813
-1440.084480	3.122003	2.326810
-1438.130422	-0.650031	2.336806
-1436.885746	5.422351	2.346803
-1434.537116	-1.581728	2.356800
-1432.545566	-2.449820	2.366797
-1430.713902	0.677077	2.376794
-1428.799881	0.650331	2.386790
-1427.031164	5.615693	2.396787
-1425.376188	10.297692	2.406784
-1423.251424	4.794692	2.416781
-1421.146229	4.678928	2.426778
-1419.305057	-0.259207	2.436774
-1417.915841	5.979520	2.446771
-1416.101561	5.379814	2.456768
-1413.602289	4.207837	2.466765
-1411.944024	2.968386	2.476762
-1410.296068	5.221569	2.486758
-1408.052345	5.931521	2.496755
-1406.175304	5.317040	2.506752
-1404.596380	5.265008	2.516749
-1402.540667	2.777757	2.526746
-1400.506635	0.357134	2.536742
-1398.859586	-1.862597	2.546739
-1396.933859	5.453925	2.556736
-1395.068328	-1.785414	2.566733
-1393.208586	5.868509	2.576730
-1391.510528	4.351130	2.586726
-1389.505632	9.866077	2.596723
-1387.389444	4.921837	2.606720
-1385.406143	1.906202	2.616717
-1383.938006	2.271383	2.626714
-1381.949275	5.707911	2.636710
-1380.057393	8.757321	2.646707
-1378.034651	9.414254	2.656704
-1376.035542	8.219744	2.666701
-1374.310258	2.303894	2.676698
-1372.579705	3.037599	2.686694
-1370.951584	6.956585	2.696691
-1368.919076	11.289260	2.706688
-1366.683073	6.600593	2.716685
-1364.760577	0.119512	2.726682
-1363.270877	2.251220	2.736678
-1361.137449	-5.013602	2.746675
-1359.292352	2.500591	2.756672
-1357.609001	5.731813	2.766669
-1355.642039	2.654082	2.776666
-1353.604752	0.133508	2.786662
-1351.878886	3.545820	2.796659
-1349.838546	1.361069	2.806656
-1348.238459	-1.668990	2.816653
-1346.221389	3.510896	2.826650
-1344.403117	2.125886	2.836646
-1342.715417	2.729106	2.846643
-1340.587403	-5.524812	2.856640
-1338.490219	3.786913	2.866637
-1337.071819	-1.157707	2.876634
-1334.716248	-3.612364	2.886630
-1333.254215	6.925208	2.896627
-1331.206358	9.637072	2.906624
-1329.186512	4.953034	2.916621
-1327.321824	2.985884	2.926618
-1325.569956	6.506159	2.936614
-1323.977902	10.042540	2.946611
-1322.028948	9.512933	2.956608
-1319.954358	17.033073	2.966605
-1317.745634	5.133160	2.976602
-1315.964219	9.120812	2.986598
-1314.524423	9.878987	2.996595
-1312.593436	7.591770	3.006592
-1310.613802	13.183465	3.016589
-1308.344616	6.075375	3.026586
-1306.731208	10.459388	3.036582
-1305.002518	6.944574	3.046579
-1303.020063	7.230660	3.056576
-1301.026963	9.693950	3.066573
-1299.172682	-1.416604	3.076570
-1297.586365	2.813857	3.086566
-1295.818417	2.089032	3.096563
-1293.631348	4.181821	3.106560
-1291.643249	4.714903	3.116557
-1289.927132	4.749941	3.126554
-1287.813204	5.832880	3.136550
-1286.218276	10.628806	3.146547
-1284.330854	10.506964	3.156544
-1282.440934	2.992230	3.166541
-1280.381013	4.538546	3.176538
-1278.664533	1.827796	3.186534
-1276.733509	3.989994	3.196531
-1275.264185	4.533473	3.206528
-1273.074114	3.850063	3.216525
-1271.065059	3.571404	3.226522
-1269.018013	1.783537	3.236518
-1267.495641	7.314230	3.246515
-1265.384409	9.414445	3.256512
-1263.476354	8.953010	3.266509
-1261.969397	2.636390	3.276506
-1260.048123	2.924408	3.286502
-1257.985089	10.064356	3.296499
-1256.152077	7.808650	3.306496
-1253.885700	4.043632	3.316493
-1252.075441	4.698360	3.326490
-1250.467355	3.658102	3.336486
-1248.884155	6.261234	3.346483
-1246.865789	8.303695	3.356480
-1245.010310	8.790144	3.366477
-1242.754669	6.989450	3.376474
-1240.825796	5.961028	3.386470
-1239.220688	2.349195	3.396467
-1237.579966	2.042658	3.406464
-1235.557031	3.533355	3.416461
-1233.498614	2.460529	3.426458
-1231.675724	7.570541	3.436454
-1229.829313	3.875896	3.446451
-1227.830651	0.930564	3.456448
-1226.148524	3.882614	3.466445
-1224.579394	3.922271	3.476442
-1222.134769	1.338217	3.486438
-1220.494599	4.649083	3.496435
-1218.603243	6.186110	3.506432
-1216.913455	-1.059717	3.516429
-1214.559856	4.181711	3.526426
-1212.717236	-7.997420	3.536422
-1211.325247	0.044124	3.546419
-1209.253432	4.863281	3.556416
-1207.123808	1.319129	3.566413
-1205.668977	8.032231	3.576410
-1203.443307	1.573820	3.586406
-1201.513870	4.277906	3.596403
-1200.053740	7.934955	3.606400
-1198.321915	1.943970	3.616397
-1196.359574	6.078035	3.626394
-1193.902413	1.183623	3.636390
-1192.111168	6.402939	3.646387
-1190.351634	6.107427	3.656384
-1188.584027	4.582226	3.666381
-1186.749740	0.742714	3.676378
-1184.781313	4.463717	3.686374
-1182.836493	5.014870	3.696371
-1181.232299	2.713725	3.706368
-1179.012759	9.865028	3.716365
-1177.119742	3.759851	3.726362
-1175.544886	3.380211	3.736358
-1173.605059	3.188499	3.746355
-1171.883918	1.763900	3.756352
-1169.796865	-3.314433	3.766349
-1167.627264	0.615977	3.776346
-1165.981733	0.561348	3.786342
-1164.291927	-0.746130	3.796339
-1162.463605	4.999376	3.806336
-1160.510739	6.078199	3.816333
-1158.472220	1.714994	3.826330
-1156.416570	3.129477	3.836326
-1154.889805	10.214786	3.846323
-1152.813106	9.072792	3.856320
-1151.202212	8.180571	3.866317
-1149.009574	2.074855	3.876314
-1147.345957	4.240466	3.886310
-1145.366476	9.227610	3.896307
-1143.305783	4.549823	3.906304
-1141.481386	10.621234	3.916301
-1139.799169	3.040356	3.926298
-1137.960050	6.384197	3.936294
-1136.136717	8.093224	3.946291
-1134.147826	7.626860	3.956288
-1132.298017	13.182644	3.966285
-1130.137917	3.256423	3.976282
-1128.458061	1.923720	3.986278
-1126.763702	4.247058	3.996275
-1125.019484	2.973536	4.006272
-1123.002775	2.071686	4.016269
-1120.874087	0.979825	4.026266
-1118.947705	-4.355392	4.036262
-1117.107597	5.273990	4.046259
-1115.309432	6.576539	4.056256
-1113.687050	-0.011082	4.066253
-1111.453493	6.031224	4.076250
-1109.799932	3.477498	4.086246
-1108.134666	5.164462	4.096243
-1106.005898	-0.536269	4.106240
-1104.001075	9.725192	4.116237
-1101.950890	4.946491	4.126234
-1100.687331	-0.202175	4.136230
-1098.758701	-4.811433	4.146227
-1096.614072	5.931348	4.156224
-1094.656449	12.350960	4.166221
-1092.666075	6.991314	4.176218
-1091.029089	4.328148	4.186214
-1088.786554	4.702294	4.196211
-1087.274209	5.644796	4.206208
-1085.748043	7.622440	4.216205
-1083.140916	3.179410	4.226202
-1081.549770	1.881455	4.236198
-1079.566433	3.844406	4.246195
-1077.917282	2.521387	4.256192
-1075.777453	1.574625	4.266189
-1074.409558	-3.957023	4.276186
-1072.427719	1.667691	4.286182
-1070.178280	4.284398	4.296179
-1068.446470	3.510262	4.306176
-1066.587182	-0.146844	4.316173
-1064.716687	1.208914	4.326170
-1062.628772	6.098266	4.336166
-1060.835540	5.101158	4.346163
-1059.142272	5.604226	4.356160
-1057.154719	2.941860	4.366157
-1055.298672	4.451513	4.376154
-1053.565534	1.979835	4.386150
-1051.548946	6.683239	4.396147
-1049.962833	0.210404	4.406144
-1047.725214	1.842197	4.416141
-1045.582400	5.699644	4.426138
-1044.237878	1.935404	4.436134
-1042.201960	4.412603	4.446131
-1040.243463	8.375320	4.456128
-1038.385083	3.076300	4.466125
-1036.751908	-4.922975	4.476122
-1034.720236	1.734315	4.486118
-1032.623754	5.387609	4.496115
-1031.056816	5.159331	4.506112
-1029.178842	-1.565423	4.516109
-1027.274386	4.082761	4.526106
-1025.286838	7.079282	4.536102
-1023.437956	3.092298	4.546099
-1021.564270	5.478618	4.556096
-1019.742686	5.119629	4.566093
-1017.824378	0.977867	4.576090
-1015.748011	1.381812	4.586086
-1013.743725	6.137743	4.596083
-1012.378602	5.840698	4.606080
-1010.448868	7.738073	4.616077
-1008.337065	3.439063	4.626074
-1006.647134	1.544318	4.636070
-1004.791641	8.700330	4.646067
-1002.803143	7.143104	4.656064
-1000.937469	9.941243	4.666061
-998.833254	7.623424	4.676058
-997.209015	9.069139	4.686054
-995.564839	4.742282	4.696051
-993.299377	5.937052	4.706048
-991.475203	1.061951	4.716045
-989.513660	1.623225	4.726042
-987.962962	4.861730	4.736038
-985.683263	1.778507	4.746035
-983.861624	4.572648	4.756032
-982.120647	8.816508	4.766029
-980.258360	5.015305	4.776026
-978.407058	3.255829	4.786022
-976.328701	8.964675	4.796019
-974.822745	9.464596	4.806016
-972.948835	11.404086	4.816013
-970.817770	5.731521	4.826010
-968.919595	6.388206	4.836006
-967.111297	5.361920	4.846003
-965.520942	6.298346	4.856000
-963.397410	11.009997	4.865997
-961.350854	15.244493	4.875994
-959.579199	8.879410	4.885990
-957.874643	-0.744891	4.895987
-955.608158	6.042300	4.905984
-954.217561	1.072339	4.915981
-952.082098	-2.235683	4.925978
-950.049663	-1.955706	4.935974
-948.429123	3.619520	4.945971
-946.566658	7.633989	4.955968
-944.639622	5.402964	4.965965
-942.666842	13.249218	4.975962
-940.709191	7.446510	4.985958
-939.244495	8.862512	4.995955
-936.838631	6.398628	5.005952
-935.337789	3.165236	5.015949
-933.609998	5.224433	5.025946
-931.436977	4.141444	5.035942
-929.244153	1.189003	5.045939
-927.849761	0.680490	5.055936
-925.927576	5.017002	5.065933
-923.917892	2.567521	5.075930
-922.180033	3.043034	5.085926
-920.377585	-0.301721	5.095923
-918.252473	4.404982	5.105920
-916.491392	8.884099	5.115917
-914.266684	0.752438	5.125914
-912.775767	3.200038	5.135910
-911.156972	-1.272702	5.145907
-908.906488	7.849167	5.155904
-907.310189	9.452569	5.165901
-905.494327	4.424125	5.175898
-903.162116	3.427818	5.185894
-901.057540	6.726263	5.195891
-899.409375	9.267155	5.205888
-897.881145	10.399873	5.215885
-895.980140	4.789411	5.225882
-893.956159	4.609743	5.235878
-892.194843	5.589943	5.245875
-890.219770	6.338610	5.255872
-888.335723	2.174003	5.265869
-886.500212	3.207083	5.275866
-884.413990	7.874248	5.285862
-882.460477	4.838526	5.295859
-881.026203	8.199926	5.305856
-878.836333	12.285275	5.315853
-877.170841	7.337727	5.325850
-875.214506	6.303637	5.335846
-873.493182	2.327681	5.345843
-871.383383	5.799001	5.355840
-869.632172	14.021788	5.365837
-867.508675	9.051563	5.375834
-865.847101	4.161492	5.385830
-863.917437	7.164250	5.395827
-861.956089	3.735718	5.405824
-860.157604	7.711539	5.415821
-858.465040	3.651771	5.425818
-856.293181	5.089003	5.435814
-854.329793	7.300074	5.445811
-852.774860	6.677524	5.455808
-850.902623	6.604252	5.465805
-848.899728	7.719554	5.475802
-846.937771	11.053478	5.485798
-845.235788	6.430114	5.495795
-843.453227	10.466916	5.505792
-841.634743	11.422228	5.515789
-839.627935	5.611743	5.525786
-837.311459	4.662226	5.535782
-835.495464	7.078448	5.545779
-833.971281	8.199223	5.555776
-832.063295	5.698179	5.565773
-830.330234	11.716560	5.575770
-828.298566	8.831019	5.585766
-826.343854	8.970371	5.595763
-824.458001	7.192860	5.605760
-822.641135	9.795267	5.615757
-820.827334	2.420928	5.625754
-819.051232	0.886749	5.635750
-817.093363	0.127195	5.645747
-815.218268	1.419265	5.655744
-813.310989	5.311422	5.665741
-811.318367	2.130561	5.675738
-809.245051	-2.294756	5.685734
-807.633269	3.443027	5.695731
-805.834210	2.847808	5.705728
-803.945827	3.814084	5.715725
-801.956198	2.948415	5.725722
-799.962479	2.045780	5.735718
-797.956013	0.206384	5.745715
-796.762236	2.812073	5.755712
-794.911671	3.847557	5.765709
-792.675340	3.371938	5.775706
-790.704122	-1.101783	5.785702
-788.911070	4.104947	5.795699
-787.072102	9.444867	5.805696
-785.122680	5.129366	5.815693
-783.176506	2.115423	5.825690
-781.353067	6.666786	5.835686
-779.621741	2.934031	5.845683
-777.626175	9.548391	5.855680
-775.759944	10.499284	5.865677
-773.928176	8.705193	5.875674
-771.653432	4.375610	5.885670
-769.974742	7.257504	5.895667
-768.297740	7.842330	5.905664
-766.628823	13.376810	5.915661
-764.447078	5.913712	5.925658
-762.451968	0.138316	5.935654
-760.743825	11.145409	5.945651
-758.649532	7.984658	5.955648
-757.426446	10.759368	5.965645
-755.052788	17.155443	5.975642
-753.093374	8.234214	5.985638
-751.202563	10.392236	5.995635
-749.500155	7.093590	6.005632
-747.746139	8.768217	6.015629
-745.535881	8.724699	6.025626
-743.692539	7.178252	6.035622
-742.194973	12.421187	6.045619
-740.165639	14.010776	6.055616
-738.224377	12.158163	6.065613
-736.250112	6.807691	6.075610
-734.571353	7.858044	6.085606
-732.677204	2.935635	6.095603
-730.747316	7.487400	6.105600
-728.821210	6.810361	6.115597
-726.929585	8.289334	6.125594
-725.054397	7.814643	6.135590
-723.027356	4.738879	6.145587
-721.441391	6.033013	6.155584
-719.496853	0.876776	6.165581
-717.614205	-2.172753	6.175578
-715.790597	4.791239	6.185574
-713.743175	4.077461	6.195571
-711.726830	2.808130	6.205568
-710.254441	5.197248	6.215565
-708.274351	3.914766	6.225562
-705.890625	0.131510	6.235558
-704.436863	2.719394	6.245555
-702.758474	0.083032	6.255552
-700.884517	10.580530	6.265549
-698.686500	2.202269	6.275546
-696.916303	-2.442943	6.285542
-695.333523	1.730103	6.295539
-693.157359	4.592573	6.305536
-691.208092	12.502818	6.315533
-689.704559	2.315541	6.325530
-687.683627	5.687549	6.335526
-685.541821	4.545036	6.345523
-683.848539	7.857291	6.355520
-682.053012	3.067516	6.365517
-679.846699	3.409949	6.375514
-677.978667	0.162261	6.385510
-676.443134	-2.002844	6.395507
-674.771746	5.309182	6.405504
-672.446175	2.523658	6.415501
-670.568601	-0.335554	6.425498
-668.675489	0.216397	6.435494
-666.674301	5.879445	6.445491
-665.256013	2.959402	6.455488
-663.562716	6.663243	6.465485
-661.070041	6.686791	6.475482
-659.427970	4.899409	6.485478
-657.627034	5.898721	6.495475
-655.449984	5.960066	6.505472
-653.763264	2.698729	6.515469
-652.043969	5.173176	6.525466
-650.160666	5.104612	6.535462
-648.009506	6.659029	6.545459
-646.121132	7.562278	6.555456
-644.359859	7.767420	6.565453
-642.362878	8.154381	6.575450
-640.755764	9.535192	6.585446
-639.147268	8.853700	6.595443
-637.015868	2.699792	6.605440
-635.116766	8.399704	6.615437
-633.098408	7.210643	6.625434
-631.064053	6.304816	6.635430
-629.250098	5.322093	6.645427
-627.638865	9.280647	6.655424
-625.675510	12.068231	6.665421
-623.935116	10.077273	6.675418
-621.742543	-0.264242	6.685414
-619.946750	0.775394	6.695411
-618.032837	7.676099	6.705408
-616.240508	10.372590	6.715405
-614.458816	9.644502	6.725402
-612.855865	10.528635	6.735398
-610.810581	5.795330	6.745395
-608.543447	5.215493	6.755392
-606.636455	2.057950	6.765389
-605.146304	8.773726	6.775386
-602.641516	1.982317	6.785382
-601.242656	11.231072	6.795379
-599.704661	15.318188	6.805376
-597.686244	12.447586	6.815373
-595.499318	10.124801	6.825370
-593.721544	4.760036	6.835366
-591.860205	8.686562	6.845363
-590.029480	7.628559	6.855360
-588.285662	13.433842	6.865357
-586.511797	19.040121	6.875354
-584.405221	15.118090	6.885350
-582.452808	13.467504	6.895347
-580.385181	3.780706	6.905344
-578.531244	15.547820	6.915341
-577.088541	11.414465	6.925338
-574.870182	7.300907	6.935334
-572.937025	5.667616	6.945331
-571.442103	18.002074	6.955328
-569.348610	12.244269	6.965325
-567.449319	13.081103	6.975322
-565.619490	11.467478	6.985318
-563.649616	10.734636	6.995315
-561.877273	4.480243	7.005312
-560.087862	9.131960	7.015309
-558.404009	8.470067	7.025306
-556.274700	9.991744	7.035302
-553.993335	8.918639	7.045299
-552.521421	13.598967	7.055296
-550.872567	4.896432	7.065293
-548.814261	3.988428	7.075290
-546.790619	10.347468	7.085286
-544.886387	11.557738	7.095283
-542.947928	6.257344	7.105280
-541.179103	11.892882	7.115277
-539.062284	10.735544	7.125274
-537.378665	8.403193	7.135270
-535.756848	3.000217	7.145267
-534.059646	2.197263	7.155264
-531.793894	7.016087	7.165261
-530.028560	7.155929	7.175258
-527.830893	9.921967	7.185254
-526.152110	6.570406	7.195251
-524.457013	6.700943	7.205248
-522.502291	11.523659	7.215245
-520.568032	10.656015	7.225242
-518.606862	4.576758	7.235238
-516.643463	6.188124	7.245235
-515.027186	8.355446	7.255232
-513.204812	6.935681	7.265229
-511.029676	2.638033	7.275226
-509.419532	8.084201	7.285222
-507.371377	8.876785	7.295219
-505.558141	9.220573	7.305216
-503.856760	3.921753	7.315213
-501.889055	7.929263	7.325210
-499.983558	8.244113	7.335206
-497.854517	7.983272	7.345203
-496.384550	8.028202	7.355200
-494.418817	9.073956	7.365197
-492.372865	12.347408	7.375194
-490.393097	3.247863	7.385190
-488.554443	2.196566	7.395187
-486.763888	7.912360	7.405184
-485.065366	4.875040	7.415181
-482.920088	2.443746	7.425178
-481.464588	3.844140	7.435174
-479.412216	3.830819	7.445171
-477.265795	4.711948	7.455168
-475.584248	9.210433	7.465165
-473.719150	6.399152	7.475162
-471.504275	7.848823	7.485158
-469.934240	3.764672	7.495155
-468.013805	4.225581	7.505152
-466.384215	7.990271	7.515149
-463.933274	6.061234	7.525146
-462.444807	8.078476	7.535142
-460.600656	7.890000	7.545139
-458.652962	7.697623	7.555136
-457.178208	10.981784	7.565133
-455.058369	6.143544	7.575130
-452.736517	1.621997	7.585126
-450.915564	6.159820	7.595123
-449.500748	3.586240	7.605120
-447.393656	1.099496	7.615117
-445.596215	2.162688	7.625114
-443.841544	3.117448	7.635110
-441.618628	5.426382	7.645107
-439.850280	12.704170	7.655104
-438.075400	6.444718	7.665101
-436.307560	7.212646	7.675098
-434.071873	1.400674	7.685094
-432.300156	1.282205	7.695091
-430.722958	4.234239	7.705088
-428.615885	-0.205626	7.715085
-426.744557	3.293129	7.725082
-424.899633	6.393475	7.735078
-422.975055	1.606964	7.745075
-421.055689	2.309659	7.755072
-419.246965	-2.126775	7.765069
-417.392159	4.549861	7.775066
-415.784432	3.202333	7.785062
-413.699403	3.117540	7.795059
-411.556093	0.585571	7.805056
-409.810229	4.563841	7.815053
-407.867556	4.575990	7.825050
-405.935541	3.620377	7.835046
-404.389329	1.305317	7.845043
-402.411491	4.553407	7.855040
-400.685313	-0.679829	7.865037
-398.698118	-0.490045	7.875034
-396.743324	1.028059	7.885030
-394.818471	1.371481	7.895027
-392.766034	7.055019	7.905024
-391.673631	6.031350	7.915021
-389.252163	3.120261	7.925018
-387.280951	4.501544	7.935014
-385.314125	-0.910624	7.945011
-383.391539	-5.453629	7.955008
-381.809777	2.537665	7.965005
-379.769442	7.256839	7.975002
-378.060481	7.731055	7.984998
-376.139250	5.406672	7.994995
-374.248396	3.785028	8.004992
-372.332550	1.123617	8.014989
-370.556345	1.634471	8.024986
-368.557126	1.484469	8.034982
-366.736466	-0.293330	8.044979
-364.746047	4.395930	8.054976
-363.012656	11.077787	8.064973
-360.994103	7.563152	8.074970
-359.227510	2.031388	8.084966
-357.343362	-0.088114	8.094963
-355.233065	-0.221100	8.104960
-353.571051	0.754834	8.114957
-351.956829	3.048913	8.124954
-349.656905	2.705665	8.134950
-347.825424	2.110353	8.144947
-346.280250	-2.470274	8.154944
-344.393213	-3.770761	8.164941
-342.005070	3.466591	8.174938
-340.466958	7.239658	8.184934
-338.640099	2.808279	8.194931
-336.822656	2.872054	8.204928
-334.991907	11.024171	8.214925
-332.954724	6.935010	8.224922
-331.027977	7.093447	8.234918
-329.008094	9.685949	8.244915
-327.286810	10.917703	8.254912
-325.728747	8.035541	8.264909
-323.744895	4.018058	8.274906
-321.420410	5.254589	8.284902
-319.811747	-0.586674	8.294899
-317.993462	1.060652	8.304896
-316.259138	6.063987	8.314893
-314.103391	3.110121	8.324890
-312.285262	1.435398	8.334886
-310.242819	4.644835	8.344883
-308.484373	0.248082	8.354880
-306.678889	-3.000395	8.364877
-304.899692	4.174716	8.374874
-302.795618	1.284370	8.384870
-300.644986	-5.846529	8.394867
-299.177749	-3.120010	8.404864
-297.441653	-1.641128	8.414861
-295.352268	-1.718618	8.424858
-293.712575	-5.003783	8.434854
-291.567681	-8.116947	8.444851
-289.659910	-2.803384	8.454848
-287.829587	-6.477388	8.464845
-286.039083	-3.767717	8.474842
-284.244775	-9.235955	8.484838
-282.180914	-9.580937	8.494835
-280.416313	-12.903395	8.504832
-278.605419	-10.253816	8.514829
-276.572767	-6.120690	8.524826
-274.709985	-9.608812	8.534822
-272.929708	-11.986406	8.544819
-271.081861	-11.172703	8.554816
-269.342937	-6.037440	8.564813
-267.389278	-8.392174	8.574810
-265.386247	-8.195333	8.584807
-263.269618	-8.264511	8.594803
-261.701327	-8.282496	8.604800
-260.067440	-5.800441	8.614797
-257.686576	-3.557590	8.624794
-256.004852	-8.433110	8.634791
-254.219726	-10.400941	8.644787
-252.370789	-8.376354	8.654784
-250.383714	-6.967490	8.664781
-248.454119	-9.244159	8.674778
-246.812021	-9.128650	8.684775
-244.934604	-10.817520	8.694771
-242.877767	-9.380309	8.704768
-240.952862	-6.834156	8.714765
-239.187032	-3.796829	8.724762
-237.250351	-1.825705	8.734759
-235.409502	-1.904534	8.744755
-233.160095	-4.780117	8.754752
-231.810756	-3.916833	8.764749
-229.987358	0.467621	8.774746
-227.787105	-2.666954	8.784743
-225.912819	-0.419023	8.794739
-224.047859	-4.865871	8.804736
-222.211933	-5.793372	8.814733
-220.672497	0.613229	8.824730
-218.471451	-5.936703	8.834727
-216.511231	-6.012461	8.844723
-214.863491	-4.004686	8.854720
-212.715754	-10.659788	8.864717
-210.913927	-1.416650	8.874714
-209.297924	-0.322747	8.884711
-207.291937	-3.232097	8.894707
-205.554696	-1.601751	8.904704
-203.274836	-0.717982	8.914701
-201.853923	-4.689752	8.924698
-199.774570	-4.400824	8.934695
-197.626972	-0.641227	8.944691
-195.957544	-5.342643	8.954688
-194.159377	-3.704642	8.964685
-192.297176	-0.820023	8.974682
-190.327003	0.591590	8.984679
-188.497779	1.953063	8.994675
-186.720595	-1.293971	9.004672
-184.537861	-3.779927	9.014669
-182.829399	5.081823	9.024666
-180.810602	3.035708	9.034663
-179.214258	3.790139	9.044659
-177.403315	3.618231	9.054656
-175.469991	7.173619	9.064653
-173.463875	8.551091	9.074650
-171.534203	1.765021	9.084647
-169.711299	3.283833	9.094643
-167.974214	-1.448887	9.104640
-166.099804	5.617991	9.114637
-164.002473	5.334086	9.124634
-162.095842	6.653230	9.134631
-160.440771	2.295177	9.144627
-158.235276	4.070323	9.154624
-156.866285	5.828931	9.164621
-154.891185	7.966100	9.174618
-152.855705	4.641564	9.184615
-150.942593	7.445464	9.194611
-149.057263	6.941186	9.204608
-147.082892	5.451656	9.214605
-145.407521	1.335109	9.224602
-143.466143	0.785578	9.234599
-141.741131	1.369508	9.244595
-139.727959	-2.235667	9.254592
-137.725933	0.039324	9.264589
-135.813789	3.422861	9.274586
-134.175181	-0.049922	9.284583
-132.275738	5.459317	9.294579
-130.229315	6.977237	9.304576
-128.314032	5.773463	9.314573
-126.772395	9.323485	9.324570
-124.782958	5.178952	9.334567
-122.783043	1.176434	9.344563
-120.843279	-5.011210	9.354560
-119.249547	8.199924	9.364557
-117.271122	4.942939	9.374554
-115.467259	4.530630	9.384551
-113.327466	3.816839	9.394547
-111.656509	4.594150	9.404544
-109.744250	3.474557	9.414541
-107.785795	8.581248	9.424538
-105.890449	1.227546	9.434535
-103.965934	1.326523	9.444531
-102.265667	-0.345033	9.454528
-100.375628	6.608883	9.464525
-98.334462	3.341905	9.474522
-96.444195	6.351599	9.484519
-94.518249	3.267213	9.494515
-92.533931	1.485616	9.504512
-91.008582	5.788255	9.514509
-89.274236	5.579685	9.524506
-87.310663	7.088753	9.534503
-84.995092	2.502231	9.544499
-83.373430	2.333745	9.554496
-81.645029	5.143483	9.564493
-79.361252	-1.504794	9.574490
-77.934496	6.171985	9.584487
-75.973144	1.476184	9.594483
-73.886842	4.143575	9.604480
-72.362990	1.216502	9.614477
-70.473363	3.313692	9.624474
-68.412074	-1.461201	9.634471
-66.453315	0.448124	9.644467
-64.435982	-1.540821	9.654464
-63.044874	2.631671	9.664461
-61.368325	8.212839	9.674458
-59.031959	1.090404	9.684455
-56.885966	-0.229060	9.694451
-55.094035	1.506358	9.704448
-53.519838	0.071259	9.714445
-51.610838	1.503798	9.724442
-49.712242	-3.382497	9.734439
-47.793604	3.200588	9.744435
-45.855015	6.639982	9.754432
-43.911832	4.392882	9.764429
-42.141031	3.995374	9.774426
-40.364678	2.599093	9.784423
-38.251808	2.761237	9.794419
-36.543481	2.479487	9.804416
-34.900960	-5.015415	9.814413
-32.677423	3.405886	9.824410
-30.672606	-0.952603	9.834407
-28.992308	-1.643559	9.844403
-27.155122	4.644641	9.854400
-25.110433	3.935044	9.864397
-23.477949	6.949596	9.874394
-21.652067	9.582780	9.884391
-19.647523	7.125386	9.894387
-17.938908	0.632051	9.904384
-15.984839	4.656367	9.914381
-13.955458	6.505526	9.924378
-12.076997	3.450881	9.934375
-10.231924	0.613141	9.944371
-8.200163	1.451403	9.954368
-6.559059	5.252483	9.964365
-4.840694	10.069134	9.974362
-3.271342	20.590588	9.984359
-1.996099	48.836821	9.994355
-0.701986	105.076469	10.004352
0.000000	156.371117	10.009357
1.117600	186.860517	10.014362
1.397293	217.037336	10.019367
2.017041	244.110169	10.024371
2.844374	255.101327	10.029376
2.700566	280.950862	10.034381
3.129990	291.824158	10.039386
2.877286	292.305312	10.044391
3.142070	315.601315	10.049395
3.733651	314.132749	10.054400
3.640096	327.702490	10.059405
3.699868	325.113940	10.064410
3.646055	332.508295	10.069415
3.874276	336.289019	10.074419
4.135258	322.364751	10.079424
3.757273	337.037999	10.084429
3.892193	331.121121	10.089434
3.966765	347.865292	10.094439
4.312283	359.376496	10.099443
4.773899	359.554498	10.104448
4.558249	360.382984	10.109453
4.427003	350.003170	10.114458
4.241419	354.404982	10.119463
4.247088	346.591127	10.124467
4.349825	345.224171	10.129472
4.126450	365.128796	10.134477
4.537071	372.565800	10.139482
4.583232	380.775295	10.144487
4.615342	382.026319	10.149491
4.852108	381.461161	10.154496
4.877244	384.681348	10.159501
4.930279	384.932395	10.164506
5.034391	391.308107	10.169511
5.220625	393.617928	10.174515
4.721489	368.321928	10.179520
4.814074	374.969132	10.184525
5.215578	381.486648	10.189530
5.303388	388.000578	10.194535
4.897719	384.432833	10.199539
5.000771	385.046490	10.204544
4.879925	403.121308	10.209549
4.839019	399.555312	10.214554
4.926938	408.358986	10.219559
4.905591	403.406871	10.224563
5.140950	408.657785	10.229568
4.992709	403.147160	10.234573
5.349312	413.833464	10.239578
5.540880	415.431226	10.244583
5.579758	415.025359	10.249587
5.652349	406.524281	10.254592
5.633740	414.617967	10.259597
5.647921	409.873074	10.264602
5.541617	423.109045	10.269607
5.854499	432.491875	10.274611
6.263421	433.916203	10.279616
5.881894	424.468813	10.284621
5.991155	421.817159	10.289626
5.585911	422.515033	10.294631
5.694546	420.811237	10.299635
5.864843	439.899392	10.304640
5.866493	444.317103	10.309645
6.461157	440.654469	10.314650
6.115564	447.994489	10.319655
6.269503	441.514709	10.324659
6.639845	451.039776	10.329664
6.275255	454.002006	10.334669
6.432831	442.011711	10.339674
6.106938	444.067317	10.344679
6.107576	442.648826	10.349683
6.251421	450.234072	10.354688
6.205612	456.553297	10.359693
6.140928	452.169478	10.364698
6.314106	463.209926	10.369703
6.325878	459.659169	10.374707
6.523019	457.728363	10.379712
5.977377	469.727130	10.384717
6.751714	477.543006	10.389722
7.020994	482.987236	10.394727
6.863264	489.393711	10.399731
6.830523	485.738081	10.404736
7.126448	493.798997	10.409741
7.263610	495.545795	10.414746
7.035333	497.076479	10.419751
7.289509	489.790627	10.424755
7.027340	478.807117	10.429760
6.812411	485.907119	10.434765
7.381468	481.747081	10.439770
7.144766	498.500067	10.444775
7.438076	500.698210	10.449779
7.677690	500.739729	10.454784
7.372564	500.801889	10.459789
7.597182	479.348481	10.464794
7.120088	490.645620	10.469799
7.012291	490.174832	10.474803
7.556088	497.270536	10.479808
7.285124	505.753030	10.484813
7.289105	493.128011	10.489818
7.731280	503.130520	10.494823
7.496667	493.380531	10.499827
7.751446	506.062246	10.504832
7.513781	504.621827	10.509837
7.789313	490.770773	10.514842
7.582433	499.183117	10.519847
7.644437	510.410067	10.524851
7.841170	505.415254	10.529856
8.103544	521.328573	10.534861
8.130391	525.642941	10.539866
8.629004	516.460413	10.544871
8.129359	509.108685	10.549875
8.341104	512.073632	10.554880
8.305148	509.604396	10.559885
8.231613	503.891005	10.564890
8.322949	512.435574	10.569895
8.455066	510.773754	10.574899
8.491778	509.966101	10.579904
8.275884	503.786550	10.584909
8.772696	515.756306	10.589914
8.697184	517.950192	10.594919
8.555978	510.370986	10.599923
8.533709	501.902327	10.604928
8.379592	507.745253	10.609933
8.715596	504.213742	10.614938
8.689135	522.975412	10.619943
8.703057	528.449344	10.624947
8.835066	530.638522	10.629952
8.382551	532.936688	10.634957
8.583640	528.712315	10.639962
8.852852	531.811607	10.644967
9.028299	532.051020	10.649971
9.075849	524.648290	10.654976
9.212332	533.568878	10.659981
9.491637	529.973861	10.664986
9.274826	530.092900	10.669991
8.675467	535.032270	10.674995
9.429536	523.227484	10.680000
8.900303	533.679825	10.685005
9.010932	546.154324	10.690010
9.220269	555.228890	10.695015
9.309906	561.435095	10.700019
9.770531	557.003741	10.705024
9.443288	566.004610	10.710029
9.832720	552.762971	10.715034
9.952337	552.848859	10.720039
9.646291	559.209630	10.725043
10.096281	551.242804	10.730048
9.963026	561.091111	10.735053
10.196036	550.266703	10.740058
9.917446	529.763964	10.745063
9.939540	528.998066	10.750067
9.917052	520.860596	10.755072
9.521948	523.368804	10.760077
9.843976	525.053008	10.765082
9.854197	542.276030	10.770087
9.789487	548.983092	10.775091
10.221325	551.324735	10.780096
10.226554	555.232544	10.785101
10.182848	550.993586	10.790106
10.111140	558.477644	10.795111
9.975277	546.485173	10.800115
10.253763	550.275285	10.805120
9.953290	559.245071	10.810125
10.437346	557.391501	10.815130
10.950321	566.994827	10.820135
10.722204	564.587765	10.825139
10.867692	553.725271	10.830144
10.663863	551.366379	10.835149
11.037726	529.786593	10.840154
10.725538	547.904721	10.845159
10.764513	537.529166	10.850163
10.986750	544.256699	10.855168
10.504921	552.883235	10.860173
10.377086	549.607037	10.865178
11.086339	567.645876	10.870183
10.825291	580.744239	10.875187
11.033798	587.395132	10.880192
11.322811	585.066451	10.885197
11.180453	582.912220	10.890202
11.227779	584.447847	10.895207
11.422960	584.270944	10.900211
11.567996	558.127543	10.905216
11.034833	562.239488	10.910221
11.065119	565.028378	10.915226
11.325205	578.278601	10.920231
11.288808	572.791076	10.925235
11.620511	575.788948	10.930240
11.252853	580.920044	10.935245
11.592894	587.251911	10.940250
11.644249	580.228599	10.945255
11.615688	588.659867	10.950259
11.748379	591.047646	10.955264
11.577405	589.263839	10.960269
11.872106	590.599164	10.965274
12.065228	584.945720	10.970279
12.094894	583.762287	10.975283
11.882701	586.703393	10.980288
11.771659	587.456860	10.985293
12.097409	583.510641	10.990298
11.864562	580.897746	10.995303
11.938118	584.452461	11.000307
12.387167	580.380923	11.005312
11.996521	584.720886	11.010317
12.038738	585.401025	11.015322
12.273454	591.648764	11.020327
12.077115	590.219092	11.025331
12.497160	588.334725	11.030336
12.310259	589.800471	11.035341
12.412020	582.553072	11.040346
12.316794	591.277253	11.045351
12.181535	598.017667	11.050355
12.690686	595.002582	11.055360
12.532370	610.885316	11.060365
12.679620	607.182028	11.065370
12.916345	606.703603	11.070375
12.570167	605.077047	11.075379
12.828613	597.479794	11.080384
12.947139	613.963370	11.085389
13.077730	604.795322	11.090394
13.055173	600.445742	11.095399
12.962757	606.140093	11.100403
13.298206	607.155101	11.105408
13.231571	614.318250	11.110413
13.014545	607.383457	11.115418
13.116668	597.133410	11.120423
13.261865	603.912681	11.125427
13.184715	609.812761	11.130432
13.040496	611.703797	11.135437
13.313778	611.107576	11.140442
13.364411	607.634166	11.145447
13.283867	616.220400	11.150451
13.435861	602.876229	11.155456
13.206593	613.260290	11.160461
13.192419	622.001526	11.165466
13.232643	612.191858	11.170471
13.069964	616.258927	11.175475
13.317109	618.417142	11.180480
13.306192	636.963587	11.185485
13.593089	630.478290	11.190490
14.040994	628.151072	11.195495
13.753503	645.685051	11.200499
14.245782	630.168689	11.205504
14.280046	637.985980	11.210509
14.552067	639.306004	11.215514
14.543700	618.368951	11.220519
13.971990	608.396668	11.225523
14.109232	602.665394	11.230528
13.748522	611.998064	11.235533
14.325272	623.254981	11.240538
14.331311	632.076581	11.245543
14.307277	637.334251	11.250547
14.274979	630.548188	11.255552
14.260693	637.002817	11.260557
14.262536	642.357290	11.265562
14.253402	636.092668	11.270567
13.846684	641.438177	11.275571
14.273586	631.629910	11.280576
14.341187	644.209130	11.285581
14.427567	636.934194	11.290586
14.298157	628.667054	11.295591
14.428740	646.536495	11.300595
14.999641	644.552368	11.305600
15.071065	659.938037	11.310605
15.140699	663.296273	11.315610
15.109743	637.280146	11.320615
14.893073	632.256597	11.325619
14.807760	627.186870	11.330624
14.757518	648.816309	11.335629
15.211006	646.633281	11.340634
15.254023	653.473026	11.345639
15.279319	661.369033	11.350643
15.091673	663.956147	11.355648
14.973003	661.525307	11.360653
15.465615	656.565261	11.365658
15.521476	651.313736	11.370663
15.470479	663.031923	11.375667
15.464826	657.635660	11.380672
15.567161	661.805564	11.385677
15.666340	656.020413	11.390682
15.643155	657.534176	11.395687
15.631979	671.559468	11.400691
15.921137	657.972594	11.405696
15.904987	662.339593	11.410701
15.904077	646.070789	11.415706
15.827397	638.973247	11.420711
15.649889	636.025079	11.425715
15.597144	635.652742	11.430720
15.362948	657.183793	11.435725
15.748652	661.903033	11.440730
16.006842	659.617103	11.445735
16.022589	664.784859	11.450739
16.021958	660.376570	11.455744
16.122625	668.304716	11.460749
16.244274	671.463843	11.465754
16.341218	666.607894	11.470759
15.907961	670.391691	11.475763
16.500344	667.804878	11.480768
16.088889	666.803751	11.485773
16.147483	662.326090	11.490778
16.310720	665.114298	11.495783
16.375984	673.866553	11.500787
16.315654	666.562958	11.505792
16.233964	686.708786	11.510797
16.511431	689.609673	11.515802
16.365119	700.806912	11.520807
16.613190	695.431676	11.525811
16.886545	692.280706	11.530816
16.606903	697.913485	11.535821
16.606930	692.508418	11.540826
16.830663	690.846161	11.545831
16.813247	695.900942	11.550835
16.891145	686.739669	11.555840
16.785457	691.658711	11.560845
16.819590	688.621587	11.565850
17.060194	681.050791	11.570855
16.709579	695.955007	11.575859
17.497132	707.190989	11.580864
17.308535	719.812708	11.585869
17.709912	706.936467	11.590874
17.585948	694.096703	11.595879
17.512458	691.991399	11.600883
17.481568	687.983752	11.605888
17.227305	682.183990	11.610893
17.439587	679.448050	11.615898
17.474464	680.197175	11.620903
17.358266	687.529118	11.625907
17.847135	693.168653	11.630912
17.721708	702.198923	11.635917
17.715115	696.998343	11.640922
17.734458	691.804668	11.645927
17.815191	704.143719	11.650931
18.282605	699.302799	11.655936
17.651666	699.205597	11.660941
17.942572	691.576310	11.665946
18.138089	688.450370	11.670951
17.946106	689.003855	11.675955
17.886058	687.413663	11.680960
18.156468	708.381758	11.685965
18.183011	716.846893	11.690970
18.354426	714.618949	11.695975
18.189797	719.173651	11.700979
18.591230	718.498641	11.705984
18.270743	701.258843	11.710989
18.410853	704.702047	11.715994
18.500280	701.411668	11.720999
18.491512	700.734263	11.726003
18.727887	699.574629	11.731008
18.392385	680.518972	11.736013
18.424189	692.066279	11.741018
18.677663	696.935932	11.746023
18.511508	709.943582	11.751027
18.807780	706.470401	11.756032
18.478429	722.311932	11.761037
18.647648	719.727148	11.766042
18.614532	711.722156	11.771047
18.528974	711.932231	11.776051
18.801058	702.115489	11.781056
18.629642	705.898540	11.786061
18.859529	704.744671	11.791066
18.998080	710.548891	11.796071
18.692885	719.270363	11.801075
19.401902	721.776786	11.806080
19.057955	731.480608	11.811085
19.525554	733.737730	11.816090
19.494849	739.275631	11.821095
19.164873	741.322466	11.826099
19.455773	739.848195	11.831104
19.629552	732.813171	11.836109
19.339867	741.369751	11.841114
19.369548	734.024958	11.846119
19.603056	740.897448	11.851123
19.674752	733.766735	11.856128
19.391013	743.140832	11.861133
19.771511	738.570811	11.866138
19.310261	736.845891	11.871143
19.551767	741.427299	11.876147
19.607935	727.114247	11.881152
19.562350	739.229037	11.886157
19.824472	740.826625	11.891162
19.558499	738.020280	11.896167
19.648064	740.664128	11.901171
20.130291	751.469428	11.906176
20.033126	758.210149	11.911181
20.558589	760.011757	11.916186
20.470350	738.486428	11.921191
19.875526	743.839893	11.926195
20.506075	731.360759	11.931200
20.200577	739.306406	11.936205
20.433327	741.189384	11.941210
20.428151	747.352441	11.946215
20.230787	733.944010	11.951219
20.666046	738.532368	11.956224
20.692855	751.507706	11.961229
20.671643	747.574195	11.966234
20.680220	736.585160	11.971239
20.385489	729.445072	11.976243
20.838890	738.482411	11.981248
20.954129	751.360066	11.986253
20.803280	742.402398	11.991258
20.856781	733.360106	11.996263
20.382915	736.003915	12.001267
20.706793	742.299005	12.006272
20.532165	758.313815	12.011277
20.647781	759.565749	12.016282
21.008480	749.380019	12.021287
20.739116	766.449191	12.026291
20.710076	759.635738	12.031296
21.041298	757.262451	12.036301
21.088893	757.169009	12.041306
21.003814	760.337468	12.046311
20.857320	757.062620	12.051315
20.806824	750.823468	12.056320
20.894884	758.204878	12.061325
21.126473	753.250155	12.066330
21.387350	750.596342	12.071335
20.993648	757.065797	12.076339
21.275368	755.996702	12.081344
21.133085	753.711541	12.086349
21.105728	760.318125	12.091354
20.963093	761.023020	12.096359
21.092256	763.859260	12.101363
21.236365	747.735955	12.106368
20.717654	738.482127	12.111373
20.964807	750.480856	12.116378
21.205757	746.082902	12.121383
20.732741	743.749557	12.126387
20.944711	737.812342	12.131392
21.105195	734.956915	12.136397
21.303859	739.354338	12.141402
21.163790	722.659770	12.146407
20.851331	727.637030	12.151411
21.199977	728.345583	12.156416
21.069900	725.990670	12.161421
20.690395	730.603296	12.166426
20.981703	722.376246	12.171431
20.798655	733.951542	12.176435
20.842103	726.629789	12.181440
20.510665	727.200783	12.186445
20.289718	728.643585	12.191450
20.886619	740.127624	12.196455
20.645445	748.876751	12.201459
21.068686	759.393411	12.206464
20.872197	756.940270	12.211469
20.753369	763.337507	12.216474
21.173390	755.395851	12.221479
20.953150	756.993090	12.226483
21.345934	754.698298	12.231488
21.137490	756.847184	12.236493
21.275672	754.618226	12.241498
21.261941	743.035059	12.246503
20.868891	735.003871	12.251507
21.126694	725.952659	12.256512
20.698189	732.336187	12.261517
20.988569	732.885293	12.266522
21.149865	722.657260	12.271527
21.035357	739.704860	12.276531
21.125343	728.201362	12.281536
20.994058	730.134506	12.286541
21.055330	730.201314	12.291546
21.122231	729.108129	12.296551
21.002525	725.780130	12.301555
20.976477	721.803241	12.306560
21.097543	724.626572	12.311565
21.265008	729.618766	12.316570
21.243095	726.746694	12.321575
21.001222	730.413250	12.326579
21.318419	732.095097	12.331584
21.118608	732.217733	12.336589
21.016914	710.197048	12.341594
21.017636	698.826083	12.346599
20.629681	706.414267	12.351603
20.957096	706.124811	12.356608
21.085309	698.117754	12.361613
20.919068	700.196821	12.366618
21.002172	702.805422	12.371623
20.798381	697.904378	12.376627
21.090977	701.238106	12.381632
21.092361	709.745097	12.386637
21.012628	702.354688	12.391642
20.860576	696.447155	12.396647
20.748993	709.062891	12.401651
20.967811	695.206493	12.406656
20.890075	703.216727	12.411661
20.509292	709.766105	12.416666
21.166629	703.382555	12.421671
20.810908	719.863031	12.426675
21.068972	721.471514	12.431680
20.650618	724.756192	12.436685
20.788908	728.504054	12.441690
21.133894	727.388601	12.446695
20.781020	737.097003	12.451699
20.951367	730.352696	12.456704
21.180339	731.821524	12.461709
21.142751	733.045846	12.466714
21.125118	711.407581	12.471719
20.689396	709.071449	12.476723
20.909279	709.570293	12.481728
20.776736	720.777968	12.486733
21.215818	734.319134	12.491738
21.287829	721.799765	12.496743
20.992942	712.435352	12.501747
20.873473	708.747763	12.506752
20.858323	715.282992	12.511757
20.945528	710.450659	12.516762
20.837497	706.630356	12.521767
20.767788	712.303780	12.526771
21.043354	700.906331	12.531776
20.929383	710.999254	12.536781
20.887082	704.624770	12.541786
20.957019	711.215816	12.546791
20.755304	715.453146	12.551795
21.207369	713.006978	12.556800
21.062381	711.135429	12.561805
20.860471	707.068315	12.566810
20.990692	707.075241	12.571815
20.853807	707.665672	12.576819
20.745203	699.800461	12.581824
20.634297	711.391043	12.586829
20.954940	723.818802	12.591834
20.807141	731.119535	12.596839
20.769038	733.126132	12.601843
21.426104	729.612757	12.606848
21.351121	733.451402	12.611853
21.093860	718.667141	12.616858
21.310274	710.912525	12.621863
21.319893	709.397955	12.626867
21.410820	703.839612	12.631872
21.098029	715.460815	12.636877
21.154633	710.316386	12.641882
21.323058	701.571187	12.646887
20.958768	707.693721	12.651891
21.049895	701.832563	12.656896
20.922090	703.405593	12.661901
20.951374	695.434815	12.666906
20.923011	691.281680	12.671911
20.973919	707.050728	12.676915
21.316876	700.411376	12.681920
20.984359	698.929290	12.686925
20.809805	674.295367	12.691930
20.920256	664.949138	12.696935
20.567753	671.640649	12.701939
20.938939	686.101735	12.706944
21.590242	696.236617	12.711949
20.975146	679.474345	12.716954
20.865144	679.868095	12.721959
20.856898	682.084395	12.726963
21.042345	667.200413	12.731968
20.823747	674.908234	12.736973
20.847769	672.453060	12.741978
21.001216	670.432998	12.746983
20.806042	680.728088	12.751987
20.749045	678.195944	12.756992
20.792220	683.570651	12.761997
20.671308	698.039259	12.767002
21.032045	709.907875	12.772007
20.808468	707.962124	12.777011
21.275590	707.270332	12.782016
21.143108	704.874804	12.787021
20.665291	693.846668	12.792026
20.881665	694.748205	12.797031
20.802414	712.422527	12.802035
20.908426	706.117434	12.807040
20.838934	705.321976	12.812045
20.845832	714.072524	12.817050
20.629138	712.753321	12.822055
20.418256	717.367439	12.827059
20.840153	711.497686	12.832064
20.943967	715.892880	12.837069
20.846403	725.692240	12.842074
20.868350	721.467994	12.847079
21.082638	718.161642	12.852083
21.041207	711.698704	12.857088
21.028546	721.833039	12.862093
21.255246	714.460780	12.867098
21.101248	712.727867	12.872103
21.089068	714.763445	12.877107
21.071232	719.226926	12.882112
20.928944	710.807246	12.887117
21.008704	711.112387	12.892122
21.211039	709.948719	12.897127
21.024426	713.412487	12.902131
20.933809	717.600561	12.907136
20.956478	711.054860	12.912141
20.957161	714.482453	12.917146
20.967860	707.646917	12.922151
20.826969	715.534761	12.927155
21.044346	712.462102	12.932160
21.343904	706.479392	12.937165
20.563815	701.410044	12.942170
20.957934	700.778781	12.947175
21.057096	703.624525	12.952179
20.942408	697.605373	12.957184
20.677124	693.750224	12.962189
20.812747	713.823588	12.967194
21.187537	716.685306	12.972199
20.900195	722.911485	12.977203
21.011297	715.035673	12.982208
21.231410	712.730576	12.987213
20.911582	700.620651	12.992218
20.734510	688.399659	12.997223
20.715547	688.428798	13.002227
21.127196	699.316280	13.007232
20.908335	707.421563	13.012237
20.826081	703.851046	13.017242
20.938484	709.973259	13.022247
21.087500	724.494256	13.027251
20.991170	707.856599	13.032256
20.976286	691.878562	13.037261
21.167558	691.509889	13.042266
20.999193	678.379167	13.047271
20.716060	680.686613	13.052275
20.952323	677.249817	13.057280
20.660118	688.388309	13.062285
20.737487	710.741834	13.067290
20.932702	709.311211	13.072295
20.591872	722.880542	13.077299
21.210083	721.737288	13.082304
20.698446	723.871439	13.087309
20.933116	726.533147	13.092314
21.136636	714.976072	13.097319
20.747586	722.992594	13.102323
21.167788	722.149007	13.107328
21.199478	720.360461	13.112333
21.051464	720.615190	13.117338
21.096075	699.248511	13.122343
20.649116	704.110013	13.127347
20.814035	709.274498	13.132352
21.149501	712.757516	13.137357
20.845143	718.971426	13.142362
21.222571	712.922677	13.147367
20.925094	701.340636	13.152371
21.007268	688.162066	13.157376
20.885431	700.345756	13.162381
20.570986	697.275906	13.167386
20.858808	701.703255	13.172391
20.798237	720.554202	13.177395
21.244218	724.873545	13.182400
21.433053	718.369941	13.187405
20.896540	710.287526	13.192410
20.880443	697.376939	13.197415
20.784144	695.432972	13.202419
21.000043	690.914446	13.207424
20.819391	690.259721	13.212429
20.855232	687.094588	13.217434
20.691974	693.249715	13.222439
20.958241	713.139813	13.227443
20.946382	720.831249	13.232448
21.249583	726.525638	13.237453
21.016132	718.655883	13.242458
21.000964	701.879918	13.247463
20.908526	701.457137	13.252467
20.802603	700.582331	13.257472
20.900278	693.398608	13.262477
21.121845	711.001302	13.267482
21.526318	698.370586	13.272487
20.818893	699.892541	13.277491
21.035780	695.105767	13.282496
20.722415	701.453573	13.287501
20.631859	693.265357	13.292506
20.854919	686.495317	13.297511
20.734993	700.697258	13.302515
21.068593	708.236611	13.307520
20.923250	719.184544	13.312525
20.839592	715.284656	13.317530
21.233779	701.042308	13.322535
20.997229	702.780917	13.327539
21.054756	701.151472	13.332544
21.141018	702.661979	13.337549
20.725408	700.557613	13.342554
20.749559	692.994520	13.347559
20.711202	697.841324	13.352563
20.963581	699.467270	13.357568
20.997002	711.023797	13.362573
20.928309	707.788595	13.367578
21.282571	691.392135	13.372583
20.903286	703.036548	13.377587
20.891509	697.090874	13.382592
20.844673	693.904230	13.387597
20.933993	696.921858	13.392602
21.232961	690.604925	13.397607
21.014851	695.112953	13.402611
21.358550	691.037684	13.407616
21.130727	685.695764	13.412621
20.940697	694.335775	13.417626
21.117440	687.729243	13.422631
20.894508	690.944902	13.427635
21.238122	688.227442	13.432640
21.152446	694.753407	13.437645
20.937191	692.479893	13.442650
20.900316	692.625432	13.447655
21.033711	695.192895	13.452659
21.293662	690.262057	13.457664
21.334649	691.582658	13.462669
20.850625	682.583538	13.467674
21.270653	685.691932	13.472679
20.995846	674.153607	13.477683
20.947500	663.426023	13.482688
20.608295	664.706323	13.487693
20.543107	669.670940	13.492698
20.697377	686.059011	13.497703
20.729070	695.319695	13.502707
20.915042	691.925610	13.507712
21.352758	694.029793	13.512717
20.800736	693.475292	13.517722
21.337653	688.990732	13.522727
21.066436	700.263085	13.527731
21.123225	689.925581	13.532736
20.974396	679.132006	13.537741
20.778958	672.628988	13.542746
20.951382	681.163881	13.547751
20.991819	695.602026	13.552755
20.934994	686.667246	13.557760
20.989072	673.065804	13.562765
20.705343	681.187725	13.567770
20.927223	684.805548	13.572775
20.440327	698.585023	13.577779
20.717044	692.814125	13.582784
21.036936	697.786731	13.587789
21.058661	695.126909	13.592794
21.317041	690.119049	13.597799
20.871730	696.164609	13.602803
21.161831	694.684163	13.607808
21.257757	695.063998	13.612813
20.971852	694.197393	13.617818
21.056723	674.477024	13.622823
20.803373	675.876101	13.627827
20.807347	670.631266	13.632832
20.734691	673.400322	13.637837
20.675487	693.865860	13.642842
20.938197	690.894788	13.647847
20.758972	706.501833	13.652851
21.493304	700.162779	13.657856
21.368274	698.757995	13.662861
21.124837	678.995355	13.667866
20.930171	675.005944	13.672871
20.911141	673.907542	13.677875
20.639134	667.952915	13.682880
21.013381	659.356273	13.687885
20.746706	666.204410	13.692890
20.986838	660.592327	13.697895
20.593256	673.016454	13.702899
20.927687	682.982656	13.707904
21.306604	690.648818	13.712909
21.199899	684.817638	13.717914
21.207160	681.964578	13.722919
20.527396	679.653174	13.727923
20.789467	670.279609	13.732928
20.933731	667.434667	13.737933
20.901857	668.601301	13.742938
21.338253	662.879069	13.747943
21.017196	662.454899	13.752947
20.998999	657.637815	13.757952
21.098623	668.382639	13.762957
20.829156	670.862950	13.767962
21.035205	666.528934	13.772967
20.897144	672.585414	13.777971
20.957197	667.129782	13.782976
21.050280	669.359884	13.787981
20.895168	675.455355	13.792986
21.054724	666.637473	13.797991
20.676209	679.571725	13.802995
20.721170	666.272950	13.808000
20.494304	672.993313	13.813005
20.670514	680.705988	13.818010
21.223804	690.720876	13.823015
20.941048	686.311835	13.828019
21.044059	679.641369	13.833024
21.096377	669.935390	13.838029
20.636706	665.802156	13.843034
21.258732	669.938075	13.848039
20.984295	682.404712	13.853043
21.023514	665.522342	13.858048
20.938419	671.169819	13.863053
20.560660	675.588180	13.868058
21.006679	671.252165	13.873063
20.721419	675.551694	13.878067
20.909156	682.996020	13.883072
21.210801	695.962175	13.888077
20.795364	696.049808	13.893082
20.941618	681.591543	13.898087
20.547172	679.356069	13.903091
20.828485	696.103948	13.908096
20.862014	705.041061	13.913101
20.926310	709.124002	13.918106
21.290515	702.232095	13.923111
20.772730	712.447764	13.928115
21.096145	705.940840	13.933120
21.162682	702.944278	13.938125
20.716108	693.705783	13.943130
20.813254	695.921048	13.948135
20.828700	707.688603	13.953139
20.925345	708.207099	13.958144
20.961824	707.760606	13.963149
21.132552	707.811536	13.968154
21.262475	707.042626	13.973159
20.990520	705.921476	13.978163
20.936436	687.920098	13.983168
20.698602	681.777084	13.988173
20.688626	706.268744	13.993178
21.035308	701.358765	13.998183
20.808706	705.221581	14.003187
21.150302	711.704649	14.008192
21.261478	702.298063	14.013210
21.214242	699.871508	14.018227
20.880844	683.821447	14.023245
20.719691	677.567143	14.028263
20.958451	684.114409	14.033280
20.761836	682.581532	14.038298
20.780083	703.459156	14.043315
21.015592	695.327949	14.048333
20.932510	701.880931	14.053351
20.769991	700.145993	14.058368
21.061053	707.087610	14.063386
21.248917	707.436043	14.068403
21.376170	705.277381	14.073421
21.305092	712.020356	14.078439
21.160861	710.755966	14.083456
21.213660	703.786434	14.088474
20.991420	704.322958	14.093491
21.673868	705.133624	14.098509
21.185683	706.744429	14.103527
21.256171	702.378498	14.108544
21.411632	708.940631	14.113562
20.828378	708.798573	14.118579
21.193564	707.572494	14.123597
20.999132	711.308735	14.128615
21.058510	707.847462	14.133632
21.487433	704.394896	14.138650
21.132274	704.161410	14.143667
21.309084	704.105778	14.148685
21.337549	707.051445	14.153703
21.169859	718.052144	14.158720
21.454511	727.354258	14.163738
21.710866	732.975403	14.168755
21.703918	731.991131	14.173773
21.550127	729.282697	14.178791
21.586659	720.006620	14.183808
21.643952	709.904572	14.188826
21.365144	718.959919	14.193843
21.385354	728.286901	14.198861
21.735621	737.416542	14.203879
21.766453	742.902199	14.208896
21.597459	732.598701	14.213914
21.406541	740.809513	14.218931
21.649404	744.818937	14.223949
21.492623	740.514404	14.228967
21.737834	744.641427	14.233984
21.587217	740.798367	14.239002
21.624394	739.121239	14.244019
21.627438	742.602634	14.249037
21.736855	736.839970	14.254055
21.849086	739.064445	14.259072
21.915817	745.293117	14.264090
21.625831	740.652759	14.269107
21.935628	738.814183	14.274125
21.348239	744.931668	14.279143
21.394162	732.453073	14.284160
22.065685	744.921257	14.289178
21.845499	769.296766	14.294195
21.874282	768.085003	14.299213
22.261955	779.352680	14.304231
21.993468	766.641057	14.309248
21.855458	765.751613	14.314266
21.912509	764.591970	14.319283
21.960850	755.801611	14.324301
22.292937	763.074904	14.329319
22.142607	767.373546	14.334336
22.461921	763.369026	14.339354
22.264619	762.872845	14.344371
21.992037	744.114569	14.349389
22.107600	743.741524	14.354407
21.976494	756.895333	14.359424
21.913209	756.731702	14.364442
21.695183	764.356982	14.369459
22.275576	756.848698	14.374477
22.252311	759.760155	14.379495
22.113049	769.342249	14.384512
22.535649	758.323065	14.389530
22.254778	774.175627	14.394547
22.142524	762.441083	14.399565
22.358179	766.019136	14.404583
22.075470	762.602964	14.409600
22.348138	759.436418	14.414618
22.228294	770.228186	14.419635
22.551506	765.219482	14.424653
22.701671	765.106753	14.429671
22.516026	773.903464	14.434688
22.773169	759.955029	14.439706
22.266906	764.444133	14.444723
22.204928	761.074557	14.449741
22.322381	759.063737	14.454759
22.385270	758.862682	14.459776
22.943485	777.611002	14.464794
22.895928	771.994477	14.469811
22.568212	763.254645	14.474829
22.837835	763.478360	14.479847
22.410807	780.239825	14.484864
22.918728	768.596709	14.489882
22.317172	763.090554	14.494899
22.887144	766.475255	14.499917
22.878987	768.549051	14.504935
22.938437	769.882201	14.509952
22.824929	760.046449	14.514970
22.784573	769.249413	14.519987
22.771253	763.218456	14.525005
22.715305	760.513289	14.530023
22.546648	774.200838	14.535040
22.776726	766.952901	14.540058
22.711503	785.652790	14.545075
22.919556	789.722832	14.550093
23.312068	788.762942	14.555111
22.929547	801.798799	14.560128
23.287437	794.486424	14.565146
23.219705	792.481535	14.570163
23.101621	772.425254	14.575181
23.023881	751.277996	14.580199
22.718890	759.565996	14.585216
23.023078	763.781144	14.590234
23.193749	777.932095	14.595251
23.287705	785.795491	14.600269
23.003905	777.902778	14.605287
23.003419	779.382337	14.610304
23.282348	783.886229	14.615322
23.189209	794.647015	14.620339
23.364176	791.263242	14.625357
23.441056	788.242740	14.630375
23.295350	780.631589	14.635392
23.520534	766.098376	14.640410
23.320833	756.982639	14.645427
23.168283	747.488953	14.650445
23.276561	753.256412	14.655463
23.250799	777.103868	14.660480
23.588589	772.066096	14.665498
23.547485	773.824258	14.670515
23.505753	761.831510	14.675533
23.616145	752.144884	14.680551
23.178743	762.564941	14.685568
23.319886	752.841950	14.690586
23.747953	761.727185	14.695603
23.289569	769.629891	14.700621
23.416709	763.972926	14.705639
23.628503	778.304504	14.710656
23.591651	785.874164	14.715674
23.750887	785.495726	14.720691
23.489080	781.036474	14.725709
23.958764	784.451330	14.730727
23.728338	779.003959	14.735744
23.670235	759.958995	14.740762
23.511787	767.979033	14.745779
23.458109	771.634643	14.750797
23.648461	778.022935	14.755815
23.523274	783.431244	14.760832
23.417553	783.850091	14.765850
23.695798	779.589428	14.770867
23.822783	785.195045	14.775885
23.815964	788.917117	14.780903
23.600842	789.686884	14.785920
23.701954	784.257425	14.790938
24.001039	781.505076	14.795955
23.831372	784.468198	14.800973
23.521035	782.473685	14.805991
23.905082	796.795116	14.811008
23.989285	797.381873	14.816026
24.052124	798.481684	14.821043
23.907495	807.616359	14.826061
24.566349	796.419475	14.831079
24.342884	795.125242	14.836096
23.918147	790.028170	14.841114
24.094495	790.678881	14.846131
24.161025	784.962363	14.851149
24.430510	780.500182	14.856167
24.231353	784.034280	14.861184
24.299365	784.648786	14.866202
24.072947	781.703393	14.871219
24.081233	783.368738	14.876237
24.310214	782.689750	14.881255
24.219377	785.061443	14.886272
24.291864	783.797093	14.891290
24.328224	776.007477	14.896307
23.957923	774.197129	14.901325
23.929103	785.524936	14.906343
24.228600	801.752155	14.911360
24.746908	801.340052	14.916378
24.707177	815.721215	14.921395
24.395439	810.945881	14.926413
24.781529	812.373235	14.931431
24.715133	804.667629	14.936448
24.194702	786.501725	14.941466
24.345325	788.147519	14.946483
24.202774	799.034162	14.951501
24.778628	803.325548	14.956519
24.583708	812.691610	14.961536
24.857528	810.239006	14.966554
24.497720	810.907580	14.971571
24.325012	807.448687	14.976589
24.771514	801.885495	14.981607
24.477878	808.890515	14.986624
24.445391	806.169015	14.991642
24.848457	802.706394	14.996659
24.833359	804.268507	15.001677
24.873481	799.356844	15.006695
24.380170	812.388357	15.011712
24.691439	804.655558	15.016730
24.432307	799.815211	15.021747
24.289135	807.966538	15.026765
24.552736	817.320830	15.031783
24.857354	833.144582	15.036800
25.011973	826.287740	15.041818
25.084904	835.378301	15.046835
25.025751	835.077159	15.051853
25.538173	831.335976	15.056871
25.362387	826.413117	15.061888
25.023691	809.794338	15.066906
25.443577	802.903070	15.071923
25.066540	810.067678	15.076941
25.029428	802.102580	15.081959
24.891947	805.305958	15.086976
25.001340	799.584172	15.091994
25.126647	795.481597	15.097011
25.154640	815.072698	15.102029
25.343007	817.121454	15.107047
25.164445	827.430282	15.112064
25.246211	830.487021	15.117082
25.478465	828.528670	15.122099
25.281681	821.112828	15.127117
25.413941	811.376272	15.132135
25.254090	809.264951	15.137152
25.460958	813.912476	15.142170
25.518853	804.126436	15.147187
25.224660	805.846312	15.152205
25.706470	808.054333	15.157223
25.486348	801.691405	15.162240
25.591514	798.699423	15.167258
25.607989	789.182688	15.172275
25.273668	797.790770	15.177293
25.483656	786.684348	15.182311
25.126680	801.436977	15.187328
25.759122	821.693023	15.192346
25.834575	818.386459	15.197363
25.644414	821.764978	15.202381
25.830144	822.908114	15.207399
25.141167	821.180037	15.212416
25.340413	828.800156	15.217434
25.629293	824.363183	15.222451
25.430571	834.587144	15.227469
25.800788	833.114867	15.232487
25.784717	831.251169	15.237504
25.746295	830.169665	15.242522
25.817113	832.660302	15.247539
25.675636	833.341250	15.252557
25.826881	829.148015	15.257575
25.675910	840.536242	15.262592
25.895099	831.418152	15.267610
25.768568	835.182921	15.272627
25.804489	831.736370	15.277645
26.114500	843.069963	15.282663
25.852401	840.268671	15.287680
25.935962	845.506864	15.292698
26.032111	851.276296	15.297715
26.216891	853.860446	15.302733
26.797315	835.314442	15.307751
26.326003	826.029621	15.312768
26.185318	824.283321	15.317786
26.320355	818.917651	15.322803
26.120182	823.985584	15.327821
26.438177	825.673904	15.332839
26.131819	818.865407	15.337856
26.028618	821.589854	15.342874
26.127497	823.223454	15.347891
26.134860	823.836623	15.352909
26.430894	834.293138	15.357927
26.370221	836.295096	15.362944
26.545523	843.437706	15.367962
26.588725	826.507902	15.372979
26.319084	825.331139	15.377997
26.437796	814.069370	15.383015
26.445564	820.195794	15.388032
26.442455	826.872929	15.393050
26.435553	829.495506	15.398067
26.469610	838.675637	15.403085
26.488973	837.035944	15.408103
26.640002	828.270064	15.413120
26.473490	832.572878	15.418138
27.132065	827.947965	15.423155
26.533589	839.794509	15.428173
26.869307	831.785670	15.433191
26.711122	824.695572	15.438208
26.453937	834.052701	15.443226
26.489212	834.033796	15.448243
26.300795	838.443922	15.453261
26.394619	837.934346	15.458279
26.629419	833.347122	15.463296
26.934876	831.979552	15.468314
26.992982	829.227871	15.473331
26.765944	838.240429	15.478349
26.872102	834.973009	15.483367
27.072534	839.574378	15.488384
26.974582	833.119597	15.493402
27.362580	831.669652	15.498419
27.014585	841.382606	15.503437
27.190550	831.595023	15.508455
27.084971	836.695065	15.513472
26.739727	849.592889	15.518490
27.026601	831.046512	15.523507
26.924202	843.581570	15.528525
26.645479	836.559451	15.533543
26.857593	850.417580	15.538560
26.935378	848.479139	15.543578
27.401352	851.413269	15.548595
27.101920	861.061863	15.553613
27.345517	857.852743	15.558631
27.214177	860.323713	15.563648
27.095908	865.046698	15.568666
27.673210	854.913534	15.573683
27.401754	866.284816	15.578701
27.674250	860.949119	15.583719
27.641780	861.876948	15.588736
27.536193	857.185125	15.593754
27.715642	862.950716	15.598771
27.614764	862.151297	15.603789
27.804978	855.282473	15.608807
27.461322	826.561872	15.613824
27.457134	838.551168	15.618842
27.798373	843.010537	15.623859
27.561622	844.681932	15.628877
27.442273	844.914195	15.633895
27.814008	847.278199	15.638912
27.702597	847.735707	15.643930
28.177633	855.322872	15.648947
27.678944	839.722129	15.653965
27.512973	827.274096	15.658983
27.818312	840.793314	15.664000
27.852107	856.496689	15.669018
27.965110	847.760456	15.674035
27.836872	850.432273	15.679053
27.921255	844.624796	15.684071
27.805922	844.897316	15.689088
27.649346	857.423723	15.694106
27.657093	856.231037	15.699123
27.590701	857.093490	15.704141
28.038126	856.277421	15.709159
28.209888	849.185031	15.714176
27.657605	853.522628	15.719194
27.859389	846.276018	15.724211
28.101638	846.337363	15.729229
28.221420	850.610258	15.734247
28.015473	849.719058	15.739264
28.179412	854.478832	15.744282
27.969162	842.953328	15.749299
28.025665	853.657262	15.754317
27.686886	853.079821	15.759335
27.939312	859.774422	15.764352
28.051597	880.308550	15.769370
28.291260	872.035013	15.774387
28.376967	876.475368	15.779405
28.236719	872.836681	15.784423
28.020227	865.867543	15.789440
28.416285	865.690435	15.794458
28.950641	866.724499	15.799475
28.354097	871.953181	15.804493
28.341352	869.950524	15.809511
28.893391	865.021698	15.814528
28.722909	876.559353	15.819546
28.586464	869.608908	15.824563
28.818628	866.573066	15.829581
28.598376	867.749486	15.834599
28.781160	872.139753	15.839616
28.533082	873.816104	15.844634
28.533667	862.643919	15.849651
28.585008	861.565401	15.854669
28.686599	857.869277	15.859687
29.037142	860.489914	15.864704
28.620440	866.471693	15.869722
28.867942	874.504130	15.874739
28.566079	862.099759	15.879757
28.605173	869.775326	15.884775
28.750992	865.232168	15.889792
28.777661	872.127940	15.894810
28.874331	859.958887	15.899827
28.873288	875.759072	15.904845
29.277006	888.487162	15.909863
29.224753	880.178375	15.914880
28.666892	878.256353	15.919898
28.776398	883.397616	15.924915
29.218853	888.894766	15.929933
29.337788	898.129039	15.934951
29.234402	902.354168	15.939968
29.119759	896.677507	15.944986
29.372708	894.007999	15.950003
29.085133	893.037006	15.955021
29.338365	893.614116	15.960039
29.292738	889.969774	15.965056
29.228261	900.183384	15.970074
29.551067	888.469021	15.975091
29.467856	892.758569	15.980109
29.399206	893.364986	15.985127
29.472543	884.691684	15.990144
29.287525	893.746339	15.995162
29.487162	893.433816	16.000179
29.482940	889.545348	16.005197
29.246252	892.341430	16.010215
29.580739	888.661641	16.015232
29.370311	888.428665	16.020250
29.359508	884.709559	16.025267
29.650343	894.479549	16.030285
29.246830	892.726390	16.035303
29.638032	881.534371	16.040320
29.344048	889.047562	16.045338
29.505541	882.812503	16.050355
29.634357	885.654116	16.055373
29.626204	902.426002	16.060391
30.088610	907.106739	16.065408
29.853292	915.176867	16.070426
30.059667	905.883025	16.075443
29.851328	896.356452	16.080461
29.919464	906.591391	16.085479
29.997376	900.789643	16.090496
29.854052	907.935905	16.095514
30.158447	911.866353	16.100531
29.925489	907.784699	16.105549
29.716280	919.182274	16.110567
29.871086	903.475679	16.115584
30.128823	904.582171	16.120602
29.960035	904.973326	16.125619
29.908190	909.525287	16.130637
29.996504	903.890190	16.135655
30.500115	903.732109	16.140672
30.198390	913.168749	16.145690
30.534886	906.448031	16.150707
30.342954	908.821708	16.155725
30.141348	906.248277	16.160743
30.685551	900.952608	16.165760
30.287785	912.542265	16.170778
30.137431	904.607752	16.175795
30.277917	903.246034	16.180813
30.208918	909.282493	16.185831
30.349704	902.566244	16.190848
30.177971	920.897909	16.195866
30.550376	917.359928	16.200883
30.578929	932.430303	16.205901
30.297541	939.233661	16.210919
30.790405	934.529750	16.215936
30.868533	936.978341	16.220954
30.959275	930.117479	16.225971
31.030780	916.868594	16.230989
30.623665	911.988886	16.236007
30.538587	898.275786	16.241024
30.606985	914.239542	16.246042
30.971891	931.869030	16.251059
31.162517	913.355199	16.256077
30.661917	912.883782	16.261095
30.484504	912.862614	16.266112
30.701807	933.575123	16.271130
30.908784	940.523971	16.276147
30.529868	940.706393	16.281165
30.689159	937.811143	16.286183
30.750714	931.060326	16.291200
30.818250	933.628580	16.296218
30.983753	932.349385	16.301235
30.990655	933.662617	16.306253
30.563683	935.587721	16.311271
31.372274	951.219556	16.316288
31.607051	955.260216	16.321306
31.520264	944.134934	16.326323
31.275624	927.115634	16.331341
31.488163	918.287982	16.336359
31.641175	912.653575	16.341376
31.217838	916.420078	16.346394
31.276150	917.034564	16.351411
31.597518	907.508456	16.356429
31.240144	914.259427	16.361447
31.536385	910.945948	16.366464
31.383678	915.150632	16.371482
31.424572	911.523947	16.376499
31.479845	905.714796	16.381517
31.435749	925.481135	16.386535
31.820171	929.474331	16.391552
31.491086	936.247541	16.396570
31.990811	932.184321	16.401587
31.980983	925.761062	16.406605
31.429722	912.594187	16.411623
31.785064	918.986120	16.416640
32.049035	920.456555	16.421658
31.922356	929.336764	16.426675
31.792712	915.751875	16.431693
31.780958	914.699145	16.436711
32.031379	913.417421	16.441728
31.935619	914.662080	16.446746
31.815933	911.721661	16.451763
31.929909	908.869821	16.456781
32.054888	913.852902	16.461799
32.027539	921.723132	16.466816
31.899296	923.171170	16.471834
31.729738	938.203930	16.476851
32.234520	935.056962	16.481869
32.025129	932.020734	16.486887
32.407728	933.878088	16.491904
32.258086	943.240159	16.496922
32.110847	941.611292	16.501939
32.366677	939.488721	16.506957
32.144502	938.666168	16.511975
32.188248	945.422401	16.516992
32.574388	940.688317	16.522010
32.404120	938.416619	16.527027
32.412598	932.440316	16.532045
32.295500	941.506192	16.537063
32.214119	935.668484	16.542080
32.108064	937.806678	16.547098
32.057984	936.006591	16.552115
32.475463	927.901293	16.557133
32.619440	938.410447	16.562151
32.470632	939.157061	16.567168
32.348525	938.658320	16.572186
32.212036	942.797506	16.577203
32.542494	951.361016	16.582221
32.778164	967.532535	16.587239
33.147119	969.234769	16.592256
32.824982	964.248685	16.597274
32.881818	972.003273	16.602291
33.113710	959.589207	16.607309
32.932459	940.871950	16.612327
32.689742	944.214834	16.617344
32.821874	940.812689	16.622362
32.766229	957.246151	16.627379
33.030788	951.702479	16.632397
32.758625	965.351658	16.637415
33.175598	965.369412	16.642432
32.740767	964.486389	16.647450
32.960723	968.932106	16.652467
33.182009	966.461114	16.657485
33.169687	963.816591	16.662503
33.057243	965.831540	16.667520
33.349847	963.135248	16.672538
33.387580	969.198756	16.677555
33.192929	965.881748	16.682573
33.007721	964.188147	16.687591
32.967605	964.445529	16.692608
33.366969	959.286193	16.697626
33.282628	961.606542	16.702643
33.459291	952.001235	16.707661
33.570862	961.373573	16.712679
33.321437	956.498591	16.717696
33.334967	956.346302	16.722714
33.620859	974.847303	16.727731
33.940553	975.220339	16.732749
33.489568	966.949918	16.737767
33.664226	965.283874	16.742784
33.761665	964.209009	16.747802
33.380044	977.052972	16.752819
33.639674	983.880189	16.757837
33.899538	985.453531	16.762855
33.733500	991.474039	16.767872
34.125332	992.828139	16.772890
34.008444	984.419490	16.777907
33.985934	981.282665	16.782925
34.263412	975.774675	16.787943
33.866407	955.559698	16.792960
33.787935	946.536192	16.797978
33.563741	962.249362	16.802995
34.064541	970.049555	16.808013
33.842112	978.185302	16.813031
33.989426	981.190723	16.818048
34.071960	985.543530	16.823066
34.057616	983.512798	16.828083
34.152095	980.796186	16.833101
33.748760	987.326434	16.838119
33.915743	978.910272	16.843136
34.159287	977.028752	16.848154
34.158383	986.492973	16.853171
34.219675	975.243381	16.858189
34.186542	991.877784	16.863207
34.236424	999.139571	16.868224
34.451151	1005.385654	16.873242
34.447846	1014.812525	16.878259
34.482286	1005.036382	16.883277
33.999100	1007.565056	16.888295
34.236256	1006.784083	16.893312
34.636930	1003.323371	16.898330
34.314107	1015.300703	16.903347
34.587258	1001.645210	16.908365
34.279307	1007.019825	16.913383
34.621193	1005.630701	16.918400
34.649828	1005.873974	16.923418
34.652496	1023.405610	16.928435
35.114943	1030.507244	16.933453
35.066893	1032.982265	16.938471
35.039263	1020.447511	16.943488
35.127620	1001.275055	16.948506
34.872416	1007.600794	16.953523
34.789611	997.789870	16.958541
35.256038	1006.213757	16.963559
35.063673	1008.007078	16.968576
35.012655	1001.499119	16.973594
34.938103	1007.366620	16.978611
35.185082	1014.988665	16.983629
35.281167	1031.896661	16.988647
35.175617	1034.490961	16.993664
35.707163	1026.353263	16.998682
35.400995	1017.992079	17.003699
35.435815	997.837169	17.008717
35.278001	996.294924	17.013735
35.105297	997.706015	17.018752
35.490088	998.708885	17.023770
35.586951	1010.762433	17.028787
35.424887	1007.080000	17.033805
35.399073	1002.822142	17.038823
35.402635	1009.196280	17.043840
35.775816	1016.762022	17.048858
35.776798	1016.017137	17.053875
35.387236	1005.347498	17.058893
35.653117	999.035969	17.063911
35.668258	1013.598913	17.068928
35.657456	1020.904995	17.073946
35.612541	1028.432022	17.078963
36.134069	1028.123222	17.083981
35.802828	1027.116711	17.088999
35.393187	1017.460137	17.094016
35.778395	1014.156044	17.099034
35.601322	1024.637806	17.104051
35.730827	1031.347370	17.109069
35.765922	1026.705416	17.114087
35.635261	1022.006526	17.119104
36.085907	1021.262295	17.124122
35.831428	1028.937570	17.129139
36.010446	1035.376548	17.134157
35.765574	1028.495226	17.139175
35.943574	1040.153618	17.144192
36.515467	1051.763366	17.149210
35.928843	1056.606714	17.154227
35.927504	1063.054016	17.159245
36.194509	1059.941792	17.164263
36.134347	1061.161911	17.169280
36.286821	1060.029500	17.174298
35.721880	1061.429211	17.179315
36.416763	1053.342530	17.184333
36.551541	1055.739637	17.189351
36.237720	1061.421945	17.194368
36.429071	1056.528551	17.199386
36.521853	1051.484137	17.204403
36.688701	1057.983268	17.209421
36.632189	1056.122844	17.214439
36.671585	1063.345438	17.219456
36.845983	1059.629787	17.224474
36.648262	1058.506029	17.229491
36.859848	1064.615786	17.234509
37.000924	1072.177671	17.239527
36.614318	1071.727394	17.244544
37.304448	1061.045992	17.249562
36.852717	1061.236879	17.254579
36.717024	1058.034716	17.259597
37.276191	1057.071832	17.264615
36.813422	1067.860302	17.269632
36.976674	1060.202882	17.274650
36.912404	1074.998773	17.279667
37.736714	1066.882008	17.284685
37.506902	1061.686113	17.289703
37.102345	1055.346189	17.294720
37.283580	1047.401193	17.299738
36.770309	1044.029582	17.304755
36.710876	1058.848280	17.309773
37.279952	1072.281617	17.314791
37.086334	1075.967484	17.319808
37.254629	1070.472151	17.324826
37.057772	1077.840963	17.329843
37.082906	1067.460651	17.334861
37.160002	1070.253920	17.339879
37.272783	1072.896782	17.344896
37.339918	1078.529360	17.349914
37.716393	1098.269769	17.354931
37.383486	1102.231109	17.359949
37.720547	1103.265194	17.364967
37.790401	1113.355288	17.369984
38.243668	1103.751391	17.375002
37.599096	1092.221012	17.380019
37.368956	1080.169954	17.385037
37.860797	1091.768905	17.390055
37.624153	1105.500640	17.395072
37.853447	1101.939819	17.400090
37.727545	1108.408577	17.405107
37.922564	1107.763306	17.410125
38.239077	1099.494690	17.415143
38.005034	1097.031789	17.420160
38.041499	1090.314786	17.425178
37.706428	1101.229209	17.430195
38.029294	1096.813476	17.435213
38.378022	1099.780513	17.440231
38.270766	1102.504085	17.445248
38.335102	1091.546499	17.450266
38.444451	1093.263405	17.455283
38.320601	1091.720452	17.460301
38.306403	1087.017127	17.465319
37.888557	1094.680734	17.470336
38.349645	1086.705248	17.475354
38.327231	1090.774375	17.480371
38.376308	1091.907864	17.485389
38.264569	1087.945253	17.490407
38.436252	1093.249709	17.495424
38.555907	1102.635008	17.500442
38.926072	1124.589695	17.505459
38.740160	1117.821624	17.510477
38.799471	1102.222850	17.515495
38.432116	1102.005454	17.520512
39.213756	1104.640766	17.525530
38.674638	1106.105575	17.530547
38.565490	1095.767105	17.535565
38.929398	1107.595681	17.540583
38.883490	1125.202826	17.545600
39.262825	1119.787079	17.550618
38.950925	1126.224156	17.555635
38.894217	1127.110249	17.560653
39.109969	1123.238551	17.565671
39.113259	1126.348766	17.570688
39.228717	1122.488343	17.575706
39.028665	1129.790051	17.580723
39.110028	1118.768381	17.585741
39.334431	1115.269685	17.590759
39.163951	1126.782370	17.595776
39.223313	1122.136516	17.600794
39.191609	1119.449438	17.605811
39.172299	1116.363983	17.610829
39.344229	1111.492544	17.615847
39.087154	1121.864437	17.620864
38.994804	1113.031802	17.625882
38.829602	1118.998746	17.630899
39.080726	1139.960988	17.635917
39.359183	1142.791374	17.640935
39.077145	1154.224342	17.645952
39.256033	1155.966346	17.650970
39.269925	1150.366616	17.655987
39.430348	1155.578509	17.661005
39.903146	1160.506212	17.666023
39.782593	1168.669864	17.671040
40.084998	1174.431705	17.676058
39.933558	1169.349115	17.681075
39.806798	1159.958797	17.686093
40.221910	1161.609650	17.691111
40.159970	1163.069160	17.696128
39.943824	1155.541402	17.701146
39.694178	1152.204806	17.706163
40.002270	1159.153366	17.711181
40.138897	1161.208850	17.716199
39.992744	1173.848697	17.721216
40.190000	1163.692554	17.726234
40.130444	1168.892339	17.731251
40.008326	1175.750634	17.736269
40.189897	1158.726018	17.741287
39.666578	1175.459245	17.746304
39.926741	1174.150777	17.751322
40.218893	1186.870181	17.756339
40.237909	1190.662170	17.761357
40.724924	1192.435269	17.766375
40.524285	1198.173514	17.771392
40.517620	1204.112066	17.776410
40.686320	1198.011004	17.781427
40.556359	1198.370807	17.786445
40.732449	1201.904942	17.791463
40.468552	1210.355744	17.796480
40.536981	1201.775845	17.801498
40.790855	1198.970854	17.806515
40.605885	1205.474242	17.811533
40.687797	1193.623442	17.816551
40.286601	1201.779954	17.821568
40.509571	1218.837822	17.826586
40.618038	1214.542760	17.831603
40.754574	1225.312858	17.836621
41.107095	1220.094834	17.841639
40.973397	1219.988042	17.846656
41.129246	1228.458439	17.851674
41.673381	1225.795922	17.856691
41.409603	1221.808755	17.861709
41.415587	1218.387335	17.866727
40.901986	1226.516167	17.871744
41.183909	1222.876139	17.876762
41.169522	1218.459093	17.881779
41.189705	1221.708207	17.886797
41.205992	1218.606043	17.891815
41.162074	1228.297506	17.896832
41.441010	1238.988279	17.901850
41.603733	1257.875799	17.906867
41.870775	1264.532080	17.911885
42.021891	1248.312891	17.916903
41.789576	1232.191042	17.921920
41.450274	1218.864243	17.926938
41.987604	1214.260120	17.931955
41.703155	1218.308146	17.936973
41.570411	1213.079414	17.941991
41.650464	1233.455588	17.947008
41.535634	1234.171630	17.952026
41.947738	1239.165667	17.957043
41.607268	1253.341962	17.962061
41.935113	1243.849210	17.967079
41.747344	1250.916210	17.972096
41.728329	1252.285514	17.977114
42.378220	1238.895343	17.982131
42.134742	1251.940889	17.987149
42.096938	1247.464647	17.992167
42.074511	1251.552698	17.997184
42.152994	1249.799711	18.002202
42.415514	1260.858063	18.007219
42.322135	1270.736767	18.012237
42.321113	1265.675776	18.017255
42.373836	1262.512736	18.022272
42.625117	1274.670869	18.027290
42.741035	1270.118197	18.032307
42.671730	1270.479340	18.037325
42.822336	1270.965866	18.042343
42.827327	1267.823020	18.047360
42.619665	1271.942187	18.052378
42.458537	1257.023343	18.057395
42.548956	1272.722859	18.062413
42.800246	1256.682744	18.067431
42.649531	1275.005211	18.072448
42.483944	1279.097221	18.077466
42.789502	1259.260575	18.082483
42.503075	1273.654789	18.087501
42.925298	1270.675075	18.092519
42.928773	1267.378314	18.097536
42.740837	1274.695466	18.102554
43.153822	1294.291893	18.107571
42.926503	1307.360081	18.112589
43.102595	1298.641832	18.117607
43.178187	1304.946411	18.122624
43.186646	1303.903014	18.127642
43.650588	1296.537299	18.132659
43.310852	1296.114147	18.137677
43.500108	1296.863500	18.142695
43.639373	1301.054771	18.147712
43.618019	1294.936783	18.152730
43.494919	1295.926282	18.157747
43.719096	1295.233882	18.162765
43.844271	1293.813222	18.167783
43.808691	1293.319546	18.172800
43.565453	1290.066840	18.177818
43.966946	1286.638966	18.182835
43.805956	1294.791833	18.187853
43.607283	1291.415615	18.192871
43.990415	1297.425757	18.197888
43.513896	1288.567758	18.202906
43.735664	1295.202958	18.207923
43.663400	1291.468379	18.212941
43.906887	1293.380999	18.217959
43.719925	1286.966949	18.222976
43.608559	1293.460212	18.227994
44.072013	1281.935468	18.233011
43.514890	1291.040266	18.238029
43.862777	1312.462385	18.243047
44.050033	1312.565539	18.248064
43.960160	1315.904584	18.253082
44.431410	1307.276119	18.258099
44.088347	1320.468169	18.263117
44.499683	1314.384998	18.268135
44.488737	1317.008308	18.273152
44.434785	1324.742998	18.278170
44.340299	1306.886044	18.283187
44.398063	1309.566037	18.288205
44.129236	1316.896108	18.293223
44.574341	1336.852417	18.298240
44.842674	1351.367462	18.303258
44.976970	1348.383307	18.308275
44.673806	1357.493269	18.313293
45.181473	1353.738560	18.318311
45.453783	1352.424995	18.323328
45.049913	1330.296190	18.328346
45.030393	1321.401478	18.333363
44.737100	1314.327963	18.338381
44.952250	1312.611379	18.343399
45.045924	1319.707468	18.348416
44.797292	1331.975252	18.353434
45.073633	1341.710105	18.358451
45.029238	1347.218998	18.363469
45.095016	1348.787151	18.368487
45.213089	1345.874798	18.373504
45.136584	1348.566771	18.378522
45.186854	1341.768798	18.383539
45.083604	1342.091310	18.388557
44.831693	1343.395511	18.393575
45.063844	1351.458979	18.398592
45.189441	1365.332973	18.403610
45.366967	1363.026198	18.408627
45.574228	1369.588239	18.413645
45.578633	1363.656453	18.418663
45.736925	1373.336218	18.423680
45.670371	1369.528349	18.428698
45.974580	1359.100182	18.433715
45.602833	1364.277458	18.438733
45.748801	1364.443825	18.443751
45.912336	1362.502655	18.448768
45.912431	1368.004462	18.453786
46.009176	1361.869188	18.458803
45.980706	1371.435585	18.463821
46.106188	1363.426947	18.468839
46.273391	1366.959395	18.473856
46.121369	1371.324551	18.478874
46.367471	1355.802687	18.483891
46.495351	1358.866343	18.488909
46.172380	1347.735939	18.493927
46.347235	1351.927842	18.498944
46.165173	1368.720133	18.503962
46.439787	1376.174366	18.508979
46.375468	1389.812822	18.513997
46.648622	1385.999543	18.519015
46.886251	1391.896072	18.524032
46.980044	1384.107984	18.529050
46.985945	1369.782170	18.534067
46.653419	1362.098253	18.539085
46.525644	1362.813219	18.544103
46.308917	1367.176107	18.549120
46.507236	1384.837433	18.554138
47.058585	1377.410549	18.559155
46.943406	1387.226740	18.564173
46.928344	1393.633904	18.569191
47.019258	1379.178120	18.574208
46.940227	1386.919988	18.579226
46.937158	1387.412147	18.584243
46.871211	1390.036375	18.589261
46.947941	1392.169084	18.594279
47.155199	1385.259541	18.599296
47.076443	1398.711541	18.604314
47.098928	1380.093365	18.609331
47.232341	1407.864043	18.614349
47.090301	1416.710818	18.619367
47.660553	1405.156364	18.624384
47.686827	1417.562858	18.629402
47.654271	1411.259414	18.634419
47.815934	1421.964304	18.639437
47.784119	1397.381884	18.644455
47.758105	1395.873635	18.649472
47.689274	1385.709429	18.654490
48.122920	1396.087782	18.659507
47.653683	1383.524029	18.664525
47.696003	1381.421284	18.669543
48.156570	1391.452417	18.674560
48.082130	1387.334336	18.679578
47.873006	1371.595603	18.684595
48.113229	1380.917811	18.689613
47.779691	1395.594941	18.694631
47.713003	1399.340874	18.699648
47.858969	1405.642141	18.704666
48.290196	1395.176391	18.709683
48.162761	1400.275396	18.714701
47.701876	1405.693418	18.719719
48.178795	1405.654428	18.724736
48.159781	1408.246007	18.729754
47.942005	1411.743897	18.734771
48.285578	1420.115259	18.739789
48.105280	1435.455417	18.744807
48.316666	1437.000361	18.749824
48.672019	1434.877582	18.754842
48.717781	1430.011998	18.759859
48.769066	1421.680099	18.764877
48.450596	1434.357087	18.769895
48.948439	1424.679806	18.774912
48.697054	1433.753244	18.779930
48.609151	1424.298354	18.784947
48.744294	1426.165346	18.789965
48.866095	1431.090909	18.794983
48.596034	1428.020203	18.800000
48.855456	1435.217336	18.805018
49.116770	1449.352919	18.810035
49.064853	1456.453413	18.815053
48.939496	1457.177436	18.820071
49.308349	1456.663312	18.825088
49.022665	1458.878988	18.830106
49.391526	1462.028512	18.835123
49.372649	1450.932911	18.840141
49.275441	1462.928117	18.845159
49.486052	1452.170310	18.850176
49.510002	1455.842028	18.855194
49.439266	1454.690123	18.860211
49.287286	1447.955812	18.865229
49.370218	1454.175914	18.870247
49.985158	1452.137584	18.875264
49.643171	1456.323840	18.880282
49.501366	1464.810377	18.885299
49.984887	1470.711775	18.890317
50.022158	1472.583368	18.895335
50.013677	1472.695711	18.900352
50.014053	1476.547377	18.905370
50.136266	1472.272070	18.910387
50.419730	1468.782750	18.915405
50.086757	1470.338992	18.920423
50.158166	1458.478640	18.925440
50.280505	1473.621141	18.930458
50.032665	1467.515599	18.935475
50.407218	1469.399479	18.940493
50.087381	1479.240501	18.945511
50.537635	1464.467778	18.950528
50.493439	1475.801723	18.955546
50.255827	1477.482762	18.960563
50.192118	1475.488148	18.965581
50.033726	1476.016088	18.970599
50.527739	1467.248618	18.975616
50.489831	1472.731356	18.980634
50.455697	1489.652784	18.985651
51.047144	1491.354214	18.990669
51.032805	1490.539387	18.995687
50.959342	1483.713886	19.000704
50.644084	1480.486777	19.005722
50.909851	1491.557372	19.010739
51.189996	1494.326212	19.015757
50.864159	1498.547658	19.020775
50.972424	1501.925938	19.025792
51.023267	1495.491180	19.030810
50.782013	1497.786296	19.035827
51.130121	1494.398350	19.040845
51.135637	1495.362634	19.045863
51.261640	1491.475263	19.050880
51.111554	1502.701841	19.055898
51.153213	1505.279044	19.060915
51.548114	1503.299390	19.065933
51.238571	1518.372374	19.070951
51.667817	1518.281210	19.075968
51.978027	1524.520159	19.080986
52.093364	1508.606841	19.086003
51.856786	1492.785835	19.091021
51.230590	1493.742308	19.096039
51.824973	1502.031252	19.101056
51.698769	1519.966291	19.106074
51.650385	1522.936962	19.111091
51.685459	1520.786588	19.116109
51.538087	1525.448357	19.121127
51.641668	1522.443897	19.126144
52.011120	1525.937842	19.131162
52.456654	1530.583725	19.136179
52.259729	1526.988516	19.141197
51.981600	1538.581613	19.146215
52.594251	1527.776946	19.151232
52.665749	1536.618060	19.156250
52.687556	1530.057352	19.161267
52.685939	1518.543657	19.166285
52.623356	1509.938848	19.171303
52.639812	1509.035736	19.176320
52.424598	1508.638338	19.181338
52.461255	1513.893693	19.186355
52.538883	1524.476775	19.191373
52.462907	1525.133151	19.196391
52.674362	1527.810701	19.201408
52.639469	1539.755134	19.206426
52.588120	1536.187048	19.211443
53.001015	1525.335582	19.216461
53.002221	1530.381085	19.221479
52.983730	1528.501952	19.226496
53.001209	1533.401713	19.231514
53.167538	1526.017272	19.236531
52.892831	1531.196435	19.241549
52.931611	1555.295222	19.246567
53.385290	1553.734064	19.251584
53.285589	1557.247768	19.256602
53.099014	1556.351859	19.261619
53.399838	1548.629774	19.266637
53.354959	1553.643307	19.271655
53.550352	1548.794724	19.276672
53.571002	1553.793089	19.281690
53.573184	1551.231092	19.286707
53.628823	1549.785314	19.291725
53.263929	1559.249746	19.296743
53.538889	1546.597073	19.301760
53.773377	1564.627241	19.306778
53.601207	1579.897040	19.311795
53.963438	1573.505407	19.316813
53.969218	1590.003724	19.321831
53.845752	1576.824654	19.326848
53.984603	1577.984767	19.331866
54.221900	1579.505146	19.336883
54.081109	1576.643462	19.341901
54.278758	1575.731905	19.346919
54.315024	1574.227865	19.351936
54.289651	1576.647450	19.356954
53.939318	1579.979321	19.361971
54.343331	1576.464461	19.366989
54.533754	1592.631311	19.372007
54.680349	1601.668135	19.377024
55.228777	1604.852769	19.382042
55.011501	1590.415242	19.387059
55.165853	1574.220343	19.392077
54.811713	1579.640285	19.397095
55.027753	1570.475045	19.402112
55.166111	1568.707754	19.407130
54.836738	1572.143250	19.412147
55.169701	1565.982808	19.417165
54.884554	1571.040951	19.422183
54.732104	1577.264031	19.427200
55.009394	1579.470184	19.432218
54.774748	1577.869337	19.437235
55.181138	1590.366384	19.442253
55.319343	1601.087732	19.447271
55.572291	1598.507764	19.452288
55.533290	1603.193178	19.457306
55.339083	1601.600038	19.462323
55.786426	1590.043015	19.467341
55.708037	1595.577873	19.472359
55.298781	1597.487648	19.477376
55.365260	1588.199949	19.482394
55.397781	1594.819844	19.487411
55.438449	1589.097696	19.492429
55.297693	1602.113018	19.497447
55.693886	1600.648327	19.502464
55.808457	1609.186879	19.507482
55.474908	1615.270533	19.512499
55.709487	1604.980714	19.517517
55.743194	1617.157312	19.522535
55.719761	1615.412667	19.527552
55.898579	1625.880585	19.532570
56.295826	1647.333085	19.537587
56.743023	1642.131278	19.542605
56.360027	1634.887858	19.547623
56.554459	1633.954787	19.552640
56.873284	1614.904441	19.557658
56.507389	1611.163902	19.562675
56.642667	1607.938858	19.567693
56.606830	1607.830616	19.572711
56.614435	1608.081186	19.577728
56.901104	1602.212051	19.582746
56.583612	1603.570776	19.587763
56.874832	1616.542401	19.592781
57.016670	1622.987571	19.597799
56.913723	1632.641524	19.602816
56.996939	1621.280967	19.607834
56.835189	1631.785890	19.612851
57.051611	1626.949659	19.617869
57.287498	1629.390518	19.622887
57.053829	1628.754591	19.627904
57.144038	1623.957363	19.632922
57.041893	1628.718923	19.637939
57.221722	1629.076529	19.642957
56.937926	1627.179124	19.647975
57.411280	1632.597704	19.652992
57.850214	1628.890855	19.658010
57.424006	1630.737268	19.663027
57.517802	1625.408554	19.668045
57.551467	1638.876672	19.673063
57.633037	1658.199240	19.678080
57.762856	1654.667520	19.683098
57.773495	1662.579287	19.688115
57.857926	1655.506724	19.693133
57.829021	1668.181003	19.698151
57.888689	1661.859598	19.703168
58.188348	1655.922301	19.708186
57.515694	1661.037544	19.713203
58.048546	1647.396670	19.718221
58.196771	1652.747546	19.723239
58.353591	1652.427680	19.728256
58.276307	1658.737913	19.733274
58.244359	1674.797162	19.738291
58.656297	1670.326944	19.743309
58.791081	1683.787631	19.748327
58.705456	1686.802028	19.753344
58.752369	1677.746276	19.758362
58.745937	1674.754606	19.763379
58.624895	1670.151502	19.768397
58.945048	1676.061731	19.773415
58.839076	1685.392933	19.778432
58.903801	1681.215611	19.783450
58.826114	1682.009124	19.788467
59.015179	1670.829073	19.793485
58.823529	1676.382808	19.798503
58.496376	1681.342289	19.803520
58.856389	1672.205941	19.808538
58.847341	1675.628138	19.813555
59.055089	1688.843593	19.818573
59.358048	1692.617967	19.823591
59.246134	1698.694630	19.828608
59.566338	1708.208013	19.833626
59.680683	1699.935115	19.838643
59.753903	1706.174178	19.843661
59.881442	1697.522424	19.848679
59.537105	1696.646942	19.853696
60.249389	1694.274512	19.858714
59.918673	1700.949228	19.863731
60.223339	1694.786166	19.868749
60.145954	1671.833968	19.873767
59.819792	1661.804198	19.878784
59.941688	1666.603195	19.883802
60.082308	1685.931329	19.888819
60.113175	1688.932657	19.893837
60.340628	1689.452565	19.898855
60.113726	1700.616823	19.903872
60.415953	1687.120441	19.908890
60.341157	1689.659614	19.913907
60.080730	1690.335969	19.918925
60.320679	1693.985891	19.923943
60.369202	1697.199919	19.928960
60.688409	1693.519224	19.933978
60.502516	1701.377403	19.938995
60.582785	1688.357661	19.944013
61.044189	1684.941382	19.949031
60.289452	1694.288729	19.954048
60.725343	1695.208786	19.959066
61.019024	1703.242191	19.964083
60.739842	1711.497509	19.969101
60.548135	1722.037162	19.974119
60.801426	1718.953732	19.979136
60.917340	1718.111044	19.984154
61.001839	1721.970598	19.989171
61.126477	1720.166150	19.994189
61.051653	1727.649542	19.999207
60.668159	1743.201756	20.004224
60.872257	1753.371568	20.009242
61.385382	1748.808111	20.014259
61.362802	1749.446544	20.019277
61.692229	1751.120572	20.024295
61.855987	1756.230688	20.029312
61.833593	1750.458753	20.034330
61.580940	1765.091107	20.039347
61.938903	1768.881114	20.044365
62.341724	1772.115746	20.049383
62.451161	1772.508964	20.054400
62.516643	1742.674412	20.059418
62.201379	1744.313591	20.064435
62.105962	1740.099649	20.069453
61.904458	1734.839218	20.074471
61.947362	1750.244009	20.079488
62.267699	1750.986646	20.084506
62.136085	1764.846977	20.089523
62.490943	1764.763743	20.094541
62.626119	1764.154731	20.099559
62.870831	1765.497763	20.104576
62.902735	1755.896919	20.109594
62.763528	1762.877769	20.114611
62.635429	1759.155118	20.119629
63.044798	1759.826141	20.124647
62.693259	1757.592653	20.129664
62.871068	1752.446347	20.134682
62.726814	1762.169895	20.139699
63.023738	1759.168379	20.144717
63.289509	1750.666019	20.149735
62.801910	1768.283807	20.154752
62.957883	1750.872455	20.159770
63.176146	1757.972490	20.164787
63.153374	1758.901188	20.169805
63.356328	1769.585595	20.174823
63.481916	1778.603856	20.179840
63.466902	1773.905944	20.184858
63.584678	1776.375100	20.189875
63.535844	1778.795313	20.194893
63.889022	1769.007948	20.199911
63.722910	1775.077555	20.204928
63.927597	1768.429374	20.209946
64.140165	1771.904351	20.214963
64.161162	1780.056786	20.219981
63.868795	1770.284259	20.224999
63.693032	1767.689246	20.230016
63.965578	1766.083801	20.235034
63.749737	1777.638840	20.240051
63.743141	1776.120376	20.245069
64.510644	1783.270493	20.250087
64.089163	1792.627688	20.255104
64.478789	1795.029117	20.260122
64.611628	1801.640977	20.265139
64.455483	1797.510638	20.270157
64.553505	1794.367003	20.275175
64.465496	1805.891456	20.280192
64.632734	1792.251326	20.285210
64.575897	1796.992345	20.290227
64.472315	1802.696473	20.295245
64.882580	1804.470882	20.300263
64.773936	1820.293971	20.305280
64.947624	1821.395851	20.310298
64.978346	1825.844480	20.315315
64.851560	1822.580947	20.320333
64.979979	1815.054534	20.325351
64.994569	1820.658813	20.330368
65.373473	1816.021566	20.335386
65.145059	1836.816663	20.340403
65.341829	1840.943078	20.345421
65.403966	1846.821370	20.350439
65.562211	1852.936822	20.355456
65.779595	1852.795281	20.360474
65.812349	1849.263260	20.365491
65.548404	1850.350762	20.370509
65.908257	1845.165958	20.375527
65.894625	1850.630809	20.380544
66.351363	1848.187414	20.385562
66.303035	1844.937322	20.390579
66.137743	1837.504136	20.395597
66.385920	1849.541334	20.400615
66.297914	1836.544359	20.405632
66.305066	1843.613600	20.410650
66.492390	1846.119658	20.415667
66.007258	1839.143328	20.420685
66.252832	1835.514453	20.425703
66.282199	1846.919545	20.430720
66.471428	1839.185999	20.435738
66.420127	1855.148641	20.440755
66.649195	1866.724050	20.445773
66.621275	1860.742944	20.450791
67.076279	1863.381724	20.455808
67.098889	1858.060344	20.460826
67.078377	1856.790281	20.465843
67.407134	1857.052572	20.470861
67.377690	1861.961499	20.475879
67.051844	1861.229354	20.480896
67.084841	1857.328401	20.485914
67.113749	1855.948206	20.490931
67.333334	1861.055750	20.495949
67.945444	1854.866411	20.500967
67.188413	1856.593344	20.505984
67.326404	1859.081314	20.511002
67.503275	1856.591301	20.516019
67.553594	1857.089907	20.521037
67.698304	1870.234566	20.526055
67.515155	1883.726469	20.531072
67.593817	1881.727189	20.536090
68.170592	1881.275074	20.541107
67.598851	1892.750091	20.546125
67.905980	1881.659598	20.551143
67.958660	1883.482381	20.556160
67.946522	1881.781523	20.561178
67.869919	1893.179951	20.566195
67.994774	1914.346716	20.571213
68.508048	1905.925932	20.576231
68.132005	1916.281174	20.581248
68.533532	1908.026080	20.586266
68.789172	1901.409829	20.591283
68.790047	1916.762507	20.596301
69.026364	1901.426464	20.601319
68.809119	1910.192716	20.606336
68.827591	1905.011984	20.611354
69.005521	1904.599080	20.616371
68.870414	1904.130692	20.621389
69.139457	1895.593118	20.626407
68.959711	1908.828087	20.631424
69.609990	1919.587579	20.636442
69.815098	1908.639967	20.641459
68.837439	1908.788077	20.646477
69.266510	1906.606287	20.651495
69.608390	1917.637545	20.656512
69.345388	1927.089899	20.661530
69.279753	1930.450389	20.666547
69.554211	1932.094663	20.671565
69.983202	1925.135354	20.676583
69.677606	1928.030709	20.681600
69.540506	1926.903505	20.686618
69.945360	1916.065619	20.691635
69.817249	1925.832322	20.696653
70.168720	1921.109749	20.701671
70.062889	1920.408591	20.706688
69.978459	1915.472364	20.711706
70.082084	1932.038058	20.716723
69.832919	1946.264175	20.721741
70.286229	1946.584478	20.726759
70.184444	1955.687084	20.731776
70.273117	1947.103517	20.736794
70.379799	1940.651007	20.741811
70.515251	1948.217395	20.746829
70.744724	1951.837592	20.751847
71.084709	1958.392899	20.756864
70.714957	1956.753772	20.761882
71.335505	1959.868785	20.766899
71.309728	1950.638826	20.771917
71.737995	1927.625262	20.776935
71.428062	1928.505372	20.781952
71.223563	1930.210283	20.786970
71.781653	1932.353629	20.791987
71.497865	1929.166232	20.797005
71.377502	1932.094978	20.802023
71.662182	1926.839544	20.807040
71.679697	1925.561838	20.812058
71.603348	1926.766519	20.817075
71.688490	1928.437833	20.822093
71.928940	1926.460730	20.827111
71.374694	1928.561984	20.832128
71.344267	1925.153283	20.837146
72.145384	1941.508670	20.842163
72.054011	1953.220189	20.847181
71.841028	1956.745759	20.852199
71.924912	1956.645167	20.857216
71.988912	1947.448875	20.862234
72.025777	1946.271908	20.867251
71.903771	1960.269327	20.872269
72.355668	1962.741872	20.877287
72.689693	1972.205247	20.882304
72.540987	1977.626399	20.887322
72.683697	1969.296913	20.892339
72.701033	1971.968531	20.897357
72.601216	1974.409491	20.902375
72.821557	1972.257826	20.907392
72.857870	1975.594206	20.912410
72.807494	1975.443445	20.917427
72.600966	1981.445644	20.922445
72.806050	1976.670885	20.927463
72.775036	2002.342858	20.932480
72.951439	1995.670769	20.937498
73.430002	1995.746361	20.942515
73.077902	2011.478694	20.947533
73.219629	1994.833070	20.952551
73.716998	2004.415148	20.957568
73.153731	2005.462290	20.962586
73.655036	2009.080061	20.967603
73.518274	2030.723676	20.972621
73.799626	2029.292989	20.977639
73.696190	2031.087197	20.982656
73.816925	2030.314513	20.987674
73.931707	2025.077482	20.992691
73.969168	2030.351773	20.997709
74.183889	2020.786103	21.002727
74.147598	2031.162764	21.007744
73.991076	2023.908992	21.012762
74.315509	2044.236328	21.017779
74.291125	2039.023840	21.022797
74.959075	2041.440715	21.027815
74.904050	2044.655599	21.032832
74.684174	2051.264033	21.037850
75.153511	2039.586740	21.042867
75.071738	2046.555421	21.047885
74.976161	2047.471363	21.052903
75.043343	2038.359455	21.057920
75.048038	2046.701054	21.062938
75.112413	2047.969828	21.067955
75.168554	2049.457792	21.072973
75.231953	2046.078150	21.077991
75.046869	2040.420135	21.083008
75.034236	2040.694390	21.088026
75.158414	2044.512308	21.093043
75.583559	2055.667258	21.098061
75.792451	2069.646631	21.103079
75.567677	2073.867069	21.108096
75.778768	2072.256447	21.113114
76.176372	2063.853230	21.118131
75.877447	2071.326910	21.123149
76.076750	2061.836822	21.128167
76.011174	2062.650448	21.133184
75.566185	2068.341471	21.138202
76.053929	2065.553303	21.143219
76.194178	2063.410463	21.148237
75.878304	2065.919709	21.153255
76.128381	2083.691621	21.158272
76.365590	2091.540753	21.163290
76.549112	2098.606380	21.168307
76.561399	2095.445675	21.173325
76.687081	2092.084408	21.178343
76.885206	2091.734351	21.183360
76.856617	2091.667423	21.188378
77.039242	2082.932722	21.193395
77.091780	2084.978150	21.198413
77.139844	2083.996027	21.203431
76.967217	2086.426590	21.208448
76.849118	2083.466800	21.213466
77.372947	2100.785285	21.218483
77.365555	2107.828658	21.223501
77.565109	2107.766255	21.228519
77.553130	2105.823084	21.233536
77.378722	2117.082329	21.238554
77.633123	2114.822174	21.243571
77.590564	2115.083897	21.248589
77.503874	2114.790264	21.253607
77.921017	2106.210864	21.258624
77.632609	2112.453489	21.263642
77.949317	2115.081334	21.268659
77.865849	2139.325645	21.273677
77.675586	2140.282646	21.278695
78.265131	2137.715777	21.283712
77.958939	2143.935294	21.288730
78.204458	2134.296209	21.293747
78.502361	2132.320931	21.298765
78.458424	2149.379979	21.303783
78.870454	2151.003132	21.308800
78.594694	2168.724486	21.313818
79.006656	2165.549594	21.318835
78.917769	2164.906288	21.323853
79.209883	2161.899166	21.328871
79.113137	2153.550336	21.333888
79.161672	2169.016812	21.338906
79.262225	2159.604545	21.343923
79.019415	2166.626489	21.348941
79.175883	2157.075525	21.353959
79.546444	2152.889420	21.358976
79.130125	2162.928765	21.363994
79.757977	2150.139075	21.369011
79.545979	2161.959663	21.374029
79.362145	2162.979353	21.379047
79.882311	2173.606403	21.384064
79.618611	2191.439913	21.389082
79.887937	2182.510418	21.394099
79.755476	2185.368779	21.399117
79.777691	2186.779577	21.404135
80.024419	2185.119999	21.409152
79.947188	2188.881187	21.414170
80.453964	2186.703486	21.419187
80.490248	2188.861641	21.424205
80.797132	2197.803277	21.429223
80.767176	2193.677874	21.434240
80.670715	2188.571999	21.439258
80.690604	2188.602741	21.444275
80.823213	2188.237172	21.449293
80.814649	2184.797394	21.454311
81.024937	2196.674958	21.459328
80.941952	2196.893575	21.464346
80.941222	2193.842683	21.469363
80.915719	2198.906049	21.474381
80.812187	2200.836369	21.479399
80.969230	2197.773693	21.484416
81.110708	2212.164315	21.489434
81.103914	2221.978731	21.494451
81.492058	2216.902554	21.499469
81.702309	2217.805140	21.504487
81.653337	2208.168126	21.509504
81.968624	2211.738525	21.514522
82.100967	2209.325558	21.519539
82.149877	2211.968589	21.524557
81.914929	2218.102841	21.529575
82.159479	2206.266974	21.534592
81.957890	2218.246408	21.539610
82.141061	2223.404722	21.544627
82.434708	2230.344309	21.549645
82.264104	2240.733095	21.554663
82.588169	2245.717144	21.559680
82.522958	2234.939814	21.564698
82.578005	2233.187301	21.569715
82.429538	2235.776857	21.574733
82.555122	2233.800724	21.579751
82.781638	2238.256804	21.584768
82.421322	2252.913890	21.589786
82.547243	2259.007139	21.594803
82.861059	2262.358332	21.599821
82.696090	2264.208787	21.604839
83.222115	2262.304094	21.609856
83.321092	2279.801440	21.614874
83.627138	2283.896402	21.619891
83.715305	2276.093790	21.624909
83.624223	2288.577946	21.629927
84.127407	2283.285188	21.634944
83.902107	2284.601742	21.639962
83.578709	2275.190923	21.644979
84.017479	2280.457954	21.649997
83.931200	2280.760473	21.655015
83.953126	2275.254205	21.660032
84.164842	2276.396466	21.665050
84.240134	2274.617910	21.670067
84.463354	2284.073987	21.675085
84.280219	2299.960601	21.680103
84.470884	2304.803906	21.685120
84.495419	2311.280672	21.690138
84.491777	2302.833534	21.695155
84.681979	2308.379325	21.700173
84.704522	2311.745507	21.705191
84.877411	2301.842591	21.710208
84.993016	2307.634675	21.715226
85.053846	2314.284208	21.720243
85.182553	2327.192714	21.725261
84.788907	2343.304863	21.730279
85.293812	2334.185906	21.735296
85.630879	2336.643005	21.740314
85.446556	2335.938610	21.745331
85.489734	2335.009949	21.750349
85.696429	2331.505139	21.755367
85.562825	2321.375776	21.760384
85.606162	2322.657367	21.765402
85.732861	2328.804009	21.770419
86.090457	2345.516100	21.775437
86.168847	2352.530182	21.780455
86.599603	2362.599000	21.785472
86.227318	2354.920101	21.790490
86.079034	2363.356278	21.795507
86.237788	2361.388211	21.800525
86.131977	2358.184139	21.805543
86.562604	2351.285723	21.810560
86.460219	2361.279082	21.815578
86.382299	2356.269301	21.820595
86.410939	2358.980090	21.825613
86.480064	2380.032140	21.830631
86.637837	2377.100669	21.835648
86.638411	2385.557173	21.840666
86.600656	2387.116777	21.845683
86.944360	2394.234881	21.850701
86.918109	2416.367218	21.855719
87.298582	2403.326504	21.860736
86.983555	2414.318936	21.865754
87.355740	2422.418098	21.870771
87.722181	2424.511849	21.875789
87.903069	2434.368850	21.880807
87.981369	2429.262558	21.885824
88.125036	2435.446655	21.890842
88.311028	2425.313458	21.895859
88.176812	2428.368004	21.900877
88.113097	2422.675543	21.905895
88.425517	2428.163351	21.910912
88.450102	2419.854803	21.915930
88.683015	2417.088324	21.920947
88.728038	2413.365432	21.925965
88.609952	2426.305508	21.930983
88.668574	2424.044272	21.936000
88.935479	2418.811950	21.941018
89.198604	2411.952011	21.946035
89.188728	2411.724781	21.951053
88.792674	2417.982338	21.956071
89.039148	2416.736518	21.961088
88.699957	2428.781324	21.966106
89.005808	2446.676934	21.971123
89.281819	2444.812081	21.976141
89.023872	2455.125275	21.981159
89.347193	2445.326490	21.986176
89.536996	2445.359246	21.991194
89.838981	2462.984908	21.996211
90.101550	2468.004798	22.001229
90.237348	2473.856655	22.006247
90.335947	2455.158894	22.011264
90.441381	2448.172270	22.016282
90.022630	2445.904551	22.021299
90.259692	2431.953004	22.026317
90.298444	2448.765605	22.031335
90.481658	2451.428169	22.036352
90.403916	2449.822655	22.041370
90.290195	2457.372404	22.046387
90.614640	2460.586657	22.051405
90.524425	2475.429797	22.056423
90.676420	2473.904066	22.061440
90.811128	2459.341906	22.066458
90.588314	2463.004455	22.071475
91.190448	2477.008834	22.076493
91.189157	2491.971532	22.081511
91.072265	2496.969340	22.086528
91.244962	2495.952373	22.091546
91.564826	2496.304197	22.096563
91.472724	2488.259629	22.101581
91.026391	2499.580613	22.106599
91.970474	2495.671881	22.111616
91.926352	2498.294401	22.116634
91.904035	2513.239235	22.121651
92.168899	2498.850570	22.126669
92.145328	2513.243422	22.131687
92.228124	2512.362708	22.136704
92.219083	2507.191655	22.141722
92.152444	2509.604603	22.146739
92.096505	2508.064039	22.151757
92.221666	2516.550311	22.156775
92.163475	2509.840666	22.161792
92.695326	2532.271984	22.166810
92.637944	2543.950240	22.171827
92.971277	2531.256735	22.176845
92.980161	2536.931419	22.181863
92.928418	2538.840940	22.186880
93.218404	2545.236945	22.191898
93.081733	2539.743278	22.196915
93.270251	2538.053614	22.201933
93.264816	2550.713120	22.206951
93.496174	2550.316067	22.211968
93.541824	2553.002156	22.216986
93.766602	2551.541899	22.222003
93.810494	2550.762563	22.227021
94.017242	2555.779584	22.232039
93.900746	2549.140571	22.237056
93.959004	2547.434704	22.242074
94.045258	2544.993635	22.247091
94.533145	2549.456908	22.252109
94.332014	2563.165470	22.257127
94.350678	2561.378604	22.262144
94.587030	2561.999386	22.267162
94.441745	2573.233886	22.272179
94.826944	2562.875333	22.277197
94.992285	2563.205387	22.282215
94.879271	2567.225658	22.287232
94.594020	2571.079104	22.292250
94.401463	2575.474676	22.297267
95.115503	2579.330839	22.302285
94.867063	2608.324127	22.307303
95.112397	2603.920312	22.312320
95.556236	2596.666498	22.317338
95.146357	2607.900734	22.322355
95.232698	2599.199955	22.327373
95.255082	2611.393350	22.332391
95.600919	2627.577479	22.337408
95.735122	2632.177400	22.342426
95.254379	2623.279128	22.347443
95.874524	2634.551316	22.352461
95.880345	2643.641913	22.357479
96.045131	2653.395440	22.362496
96.336424	2652.921183	22.367514
96.097998	2667.962771	22.372531
96.257292	2656.614451	22.377549
96.694518	2653.256873	22.382567
96.534579	2659.718370	22.387584
96.931777	2677.778258	22.392602
97.144970	2675.490766	22.397619
97.524932	2675.532535	22.402637
97.317206	2678.384899	22.407655
97.632636	2680.574921	22.412672
97.881675	2655.853563	22.417690
97.451053	2644.561549	22.422707
97.487551	2634.144484	22.427725
97.823685	2649.101528	22.432743
97.637773	2660.585630	22.437760
97.765482	2663.995695	22.442778
97.801757	2666.175946	22.447795
97.946966	2652.878335	22.452813
98.045877	2654.559338	22.457831
97.987147	2654.792185	22.462848
97.926062	2658.592608	22.467866
97.898888	2677.218069	22.472883
98.412497	2683.189118	22.477901
98.482051	2686.440915	22.482919
98.652616	2683.766921	22.487936
98.712462	2679.659313	22.492954
98.579898	2687.549633	22.497971
99.189462	2676.872054	22.502989
99.184236	2681.857627	22.508007
98.805139	2688.122033	22.513024
99.396486	2690.334140	22.518042
99.357850	2714.066478	22.523059
99.388161	2715.476037	22.528077
99.378464	2716.202129	22.533095
99.500230	2721.263434	22.538112
99.434494	2714.945050	22.543130
99.286117	2716.143972	22.548147
99.744722	2724.546526	22.553165
99.688774	2735.274497	22.558183
99.677376	2738.579329	22.563200
100.349266	2725.428941	22.568218
100.122110	2739.323521	22.573235
100.129806	2745.572692	22.578253
100.371002	2737.646325	22.583271
100.316738	2740.920235	22.588288
100.654767	2751.792281	22.593306
100.274158	2766.469632	22.598323
100.839523	2763.922250	22.603341
100.713408	2763.264400	22.608359
100.646927	2769.110083	22.613376
101.034100	2766.823943	22.618394
101.100101	2781.592145	22.623411
101.405781	2791.212391	22.628429
101.302528	2795.148575	22.633447
101.358905	2792.620196	22.638464
101.445648	2789.445896	22.643482
101.548300	2794.045393	22.648499
101.748215	2786.141314	22.653517
101.787439	2791.213444	22.658535
101.630995	2808.308505	22.663552
102.304041	2816.717040	22.668570
102.361461	2819.966082	22.673587
102.371584	2818.861743	22.678605
102.355963	2812.624212	22.683623
102.180806	2816.386228	22.688640
102.719276	2811.690197	22.693658
102.443865	2815.320314	22.698675
102.970648	2830.786759	22.703693
102.976020	2831.976123	22.708711
102.861452	2833.437110	22.713728
102.957611	2827.032297	22.718746
103.133371	2826.305077	22.723763
103.133518	2830.507962	22.728781
103.632860	2831.156049	22.733799
103.156270	2839.215357	22.738816
103.504348	2839.778223	22.743834
103.578259	2853.597380	22.748851
103.654345	2862.894014	22.753869
103.980008	2856.961531	22.758887
104.027538	2866.613545	22.763904
104.256213	2859.279063	22.768922
104.170488	2858.722533	22.773939
103.915696	2869.114961	22.778957
104.412632	2879.544081	22.783975
104.723618	2887.268613	22.788992
104.531675	2879.677099	22.794010
104.276903	2888.810968	22.799027
104.742530	2886.602763	22.804045
104.857505	2887.249205	22.809063
104.907692	2906.362118	22.814080
104.998846	2917.353882	22.819098
105.210492	2911.300326	22.824115
105.201007	2916.609954	22.829133
105.549252	2907.119959	22.834151
105.032308	2922.362747	22.839168
105.431911	2917.204273	22.844186
105.700073	2935.870291	22.849203
105.650650	2940.387888	22.854221
105.933643	2926.774656	22.859239
105.977731	2934.287691	22.864256
106.080983	2922.044288	22.869274
106.260024	2927.387578	22.874291
106.426894	2924.197329	22.879309
106.372572	2922.650170	22.884327
106.294278	2931.676483	22.889344
106.641247	2941.290247	22.894362
106.385035	2952.600932	22.899379
106.587779	2958.812804	22.904397
106.677877	2950.561945	22.909415
106.807343	2958.681229	22.914432
107.078444	2963.089522	22.919450
107.124423	2977.546470	22.924467
107.555676	2984.523479	22.929485
107.514015	2979.731100	22.934503
107.628937	2981.686475	22.939520
107.551479	2983.314614	22.944538
107.623811	2978.687341	22.949555
107.782685	2997.424352	22.954573
107.921380	2996.466263	22.959591
107.876290	3002.999274	22.964608
108.292738	3007.889413	22.969626
108.297218	3004.301839	22.974643
108.094296	3008.430171	22.979661
108.584768	3011.514248	22.984679
108.720032	3025.565276	22.989696
108.968724	3019.792883	22.994714
108.976261	3018.929645	22.999731
108.976881	3022.415905	23.004749
109.453185	3012.639552	23.009767
109.114659	3021.143407	23.014784
109.327664	3019.173685	23.019802
109.420848	3013.607008	23.024819
109.605711	3017.492597	23.029837
109.522757	3007.827434	23.034855
109.703134	3020.963515	23.039872
110.028315	3031.724548	23.044890
110.050527	3041.731544	23.049907
110.005497	3038.365027	23.054925
110.161007	3040.133805	23.059943
109.965530	3042.786845	23.064960
110.333681	3028.905080	23.069978
110.503552	3033.438874	23.074995
110.540291	3037.374829	23.080013
110.943068	3044.601044	23.085031
110.609187	3062.000005	23.090048
110.890758	3060.367029	23.095066
111.018296	3057.926373	23.100083
111.067500	3065.048499	23.105101
111.533157	3070.190398	23.110119
111.480171	3061.711357	23.115136
111.235142	3058.514379	23.120154
111.082010	3061.992910	23.125171
111.239945	3072.350358	23.130189
111.875855	3075.799064	23.135207
111.444713	3094.649144	23.140224
111.903438	3091.904750	23.145242
111.558963	3094.698760	23.150259
111.159522	3105.980481	23.155277
111.899200	3110.377831	23.160295
111.939591	3119.817191	23.165312
112.408003	3123.242269	23.170330
112.933251	3134.968914	23.175347
112.733675	3146.279371	23.180365
112.988387	3151.016783	23.185383
112.998441	3147.565943	23.190400
112.998788	3145.335912	23.195418
113.075071	3151.892903	23.200435
113.018163	3153.033227	23.205453
113.452071	3141.304864	23.210471
113.206608	3146.117296	23.215488
113.436613	3150.281267	23.220506
113.670342	3167.194976	23.225523
113.595364	3167.512230	23.230541
113.733363	3159.035723	23.235559
113.604973	3170.387553	23.240576
114.182257	3184.207006	23.245594
114.119662	3192.737765	23.250611
114.333476	3204.269478	23.255629
114.634042	3194.714532	23.260647
114.675253	3201.686967	23.265664
114.560024	3196.776452	23.270682
114.895890	3191.367673	23.275699
115.001090	3210.517838	23.280717
115.150179	3209.762601	23.285735
114.880383	3223.237300	23.290752
115.241088	3214.528599	23.295770
115.273904	3217.054813	23.300787
114.807163	3228.515693	23.305805
115.469071	3233.065500	23.310823
115.529967	3248.225154	23.315840
115.774733	3245.970300	23.320858
115.969576	3247.011498	23.325875
116.116422	3243.526241	23.330893
116.488399	3244.720910	23.335911
115.968717	3262.818360	23.340928
116.479105	3265.202368	23.345946
116.825915	3265.291121	23.350963
116.622897	3273.225239	23.355981
116.945203	3263.846133	23.360999
116.639115	3273.444664	23.366016
116.791460	3282.475328	23.371034
116.813860	3275.033505	23.376051
116.956656	3289.948877	23.381069
117.375405	3295.077883	23.386087
117.399009	3302.978247	23.391104
117.212890	3290.210365	23.396122
117.779174	3286.389203	23.401139
117.499106	3303.156860	23.406157
117.940261	3298.864001	23.411175
117.847441	3317.628176	23.416192
117.985383	3314.149829	23.421210
118.251466	3310.258527	23.426227
118.222422	3314.548014	23.431245
118.635750	3314.408267	23.436263
118.400085	3319.076026	23.441280
118.352431	3330.715601	23.446298
119.258527	3338.083551	23.451315
118.672692	3344.809118	23.456333
118.734478	3337.777899	23.461351
118.966809	3343.337037	23.466368
119.128563	3335.662936	23.471386
119.491847	3347.590208	23.476403
119.080443	3373.281969	23.481421
119.448260	3364.850514	23.486439
119.346075	3373.277561	23.491456
119.047909	3380.675477	23.496474
119.544545	3387.974218	23.501491
119.588411	3393.380136	23.506509
120.046490	3399.017367	23.511527
120.203024	3412.742857	23.516544
120.280654	3420.944606	23.521562
120.558392	3420.248299	23.526579
120.415679	3417.733460	23.531597
121.112000	3405.749089	23.536615
121.144520	3414.857148	23.541632
120.955989	3417.997647	23.546650
121.284283	3424.087442	23.551667
121.255455	3442.763698	23.556685
121.605559	3447.691311	23.561703
121.748893	3445.859289	23.566720
122.009405	3441.839046	23.571738
122.084209	3435.931380	23.576755
122.097551	3443.440925	23.581773
122.260692	3434.898107	23.586791
122.199267	3434.292842	23.591808
122.244390	3436.569341	23.596826
122.422421	3432.443468	23.601843
122.478272	3440.536998	23.606861
122.446867	3437.366449	23.611879
122.945300	3440.736474	23.616896
122.722300	3464.217018	23.621914
122.758230	3460.801312	23.626931
122.854479	3467.773752	23.631949
122.948935	3463.973489	23.636967
123.135144	3467.078641	23.641984
123.290094	3489.341829	23.647002
123.614498	3484.168403	23.652019
123.413298	3493.009343	23.657037
123.789157	3488.354760	23.662055
123.601453	3500.046689	23.667072
123.567163	3500.019994	23.672090
123.837261	3513.362474	23.677107
123.899713	3518.813461	23.682125
124.194626	3515.406798	23.687143
124.496491	3513.729635	23.692160
124.423813	3532.626176	23.697178
124.982254	3526.022285	23.702195
124.810017	3543.706767	23.707213
124.925660	3544.595420	23.712231
125.363588	3535.422688	23.717248
125.176819	3535.882847	23.722266
125.118345	3530.805843	23.727283
125.114483	3541.083222	23.732301
125.530359	3553.060490	23.737319
125.550896	3554.575525	23.742336
126.001829	3562.489715	23.747354
126.113080	3560.224634	23.752371
126.054382	3557.938662	23.757389
126.183068	3556.234038	23.762407
126.055873	3554.723602	23.767424
126.181977	3577.778165	23.772442
126.641974	3576.868721	23.777459
126.423144	3578.078156	23.782477
126.789825	3577.533645	23.787495
126.961643	3577.926412	23.792512
127.068076	3591.545995	23.797530
127.655209	3589.312814	23.802547
127.619932	3600.591134	23.807565
127.568607	3593.263167	23.812583
127.644900	3590.010124	23.817600
127.951150	3606.227615	23.822618
127.717776	3606.170514	23.827635
127.766982	3610.848802	23.832653
128.149011	3605.449820	23.837671
128.247933	3603.473037	23.842688
127.906891	3615.712621	23.847706
128.083786	3621.905300	23.852723
128.460268	3634.721973	23.857741
128.304047	3633.039948	23.862759
128.790940	3652.704880	23.867776
128.650590	3658.857686	23.872794
128.960836	3653.083887	23.877811
128.911106	3658.054075	23.882829
128.939373	3672.383951	23.887847
129.213108	3681.461588	23.892864
128.930119	3696.486946	23.897882
129.393287	3694.466242	23.902899
129.576378	3699.857944	23.907917
129.730434	3713.679297	23.912935
129.909240	3707.168101	23.917952
130.050847	3706.742066	23.922970
130.237144	3728.124292	23.927987
130.141313	3740.401193	23.933005
130.374805	3740.557577	23.938023
130.944276	3738.129741	23.943040
130.605778	3737.920268	23.948058
130.936476	3746.538900	23.953075
131.234715	3755.286216	23.958093
131.084484	3761.690795	23.963111
131.424561	3763.459346	23.968128
131.016578	3767.969066	23.973146
131.507915	3750.260373	23.978163
131.766479	3763.936888	23.983181
131.728797	3782.536324	23.988199
132.259628	3783.478373	23.993216
131.946883	3794.524960	23.998234
132.494572	3790.772717	24.003251
132.294205	3790.973094	24.008269
132.233856	3791.184190	24.013287
132.416089	3795.429909	24.018304
132.374536	3808.856956	24.023322
133.011694	3794.637378	24.028339
132.695151	3810.207846	24.033357
132.941969	3814.706805	24.038375
133.446865	3818.160849	24.043392
133.071407	3835.924493	24.048410
133.059329	3845.162648	24.053427
133.354680	3838.672147	24.058445
133.621943	3839.175572	24.063463
133.820965	3847.418780	24.068480
134.102127	3866.108304	24.073498
134.333524	3859.639003	24.078515
134.222144	3855.001409	24.083533
134.150170	3860.559699	24.088551
135.030870	3877.149254	24.093568
134.426931	3882.988235	24.098586
134.812403	3888.346171	24.103603
134.869027	3895.280293	24.108621
134.771543	3886.755949	24.113639
134.944090	3903.230296	24.118656
134.920185	3915.671301	24.123674
135.463454	3912.505008	24.128691
135.213429	3918.033491	24.133709
135.400046	3938.945551	24.138727
136.152524	3935.205464	24.143744
136.195024	3947.595791	24.148762
136.188676	3942.020244	24.153779
136.387235	3941.161113	24.158797
135.961330	3955.631321	24.163815
136.554001	3961.014466	24.168832
136.472427	3974.986122	24.173850
137.088030	3972.608323	24.178867
136.857679	3976.530470	24.183885
137.284254	3995.659536	24.188903
137.698462	3995.510996	24.193920
137.723070	3996.993961	24.198938
137.739801	3994.466977	24.203955
138.015381	3998.327355	24.208973
137.787171	3989.192099	24.213991
138.156494	3989.600593	24.219008
137.984951	3997.623695	24.224026
138.409604	3984.104905	24.229043
138.274518	3988.399694	24.234061
138.404615	3982.124275	24.239079
138.732024	3989.627299	24.244096
138.491580	3999.027037	24.249114
138.633723	4001.482464	24.254131
139.152918	4009.061124	24.259149
138.763993	4004.280502	24.264167
139.053386	4006.836750	24.269184
139.013921	4030.589445	24.274202
139.578480	4029.531149	24.279219
139.519934	4022.100279	24.284237
139.549300	4038.449710	24.289255
140.025144	4041.810895	24.294272
139.878851	4058.177338	24.299290
140.159641	4061.509048	24.304307
140.407535	4059.495083	24.309325
140.250966	4055.862912	24.314343
140.689759	4072.442899	24.319360
140.476721	4084.462650	24.324378
140.948977	4089.587346	24.329395
140.968667	4085.032625	24.334413
140.954456	4088.916412	24.339431
141.127751	4089.554400	24.344448
140.999216	4104.767165	24.349466
141.431235	4102.180252	24.354483
141.500832	4112.764923	24.359501
141.672789	4128.921802	24.364519
142.043260	4130.061723	24.369536
142.305074	4142.528961	24.374554
142.355697	4129.124732	24.379571
142.563486	4125.334552	24.384589
142.396805	4140.698970	24.389607
142.901789	4156.343373	24.394624
142.886416	4163.214366	24.399642
142.943032	4162.806588	24.404659
143.116600	4166.714741	24.409677
143.132098	4164.832997	24.414695
143.402171	4179.507930	24.419712
143.440382	4192.269672	24.424730
143.585528	4186.504680	24.429747
143.743362	4182.364511	24.434765
143.699493	4198.070494	24.439783
143.747397	4204.731603	24.444800
143.856599	4212.953937	24.449818
144.325318	4216.098390	24.454835
144.966364	4232.873667	24.459853
144.896065	4237.113359	24.464871
145.240288	4236.337193	24.469888
145.113008	4241.057976	24.474906
145.250393	4238.470022	24.479923
145.528446	4234.929004	24.484941
145.322112	4241.686513	24.489959
145.230562	4232.744868	24.494976
145.520380	4251.851230	24.499994
145.906868	4248.363724	24.505011
146.144559	4250.788229	24.510029
146.241111	4249.971302	24.515047
146.426432	4247.116888	24.520064
146.660027	4248.389561	24.525082
146.593174	4246.181089	24.530099
147.057401	4247.560958	24.535117
146.847621	4249.724031	24.540135
146.770213	4250.015733	24.545152
147.181717	4267.502613	24.550170
147.144739	4280.125375	24.555187
147.274658	4279.040377	24.560205
147.188189	4280.795963	24.565223
147.266900	4286.162042	24.570240
147.728454	4298.955511	24.575258
147.274077	4307.448677	24.580275
147.910799	4313.628923	24.585293
147.863956	4336.292160	24.590311
147.996547	4334.839351	24.595328
148.208752	4341.541985	24.600346
148.287397	4359.274774	24.605363
148.727032	4359.904145	24.610381
148.847597	4363.183586	24.615399
149.308710	4376.652956	24.620416
149.281188	4389.667647	24.625434
149.456007	4395.373241	24.630451
149.871659	4382.058489	24.635469
149.696359	4390.844702	24.640487
149.965646	4382.204173	24.645504
150.227778	4390.535178	24.650522
150.377399	4403.760008	24.655539
150.255936	4403.338131	24.660557
150.209171	4403.806676	24.665575
150.901874	4403.686115	24.670592
150.838232	4410.099985	24.675610
150.789117	4419.034451	24.680627
151.469828	4419.917256	24.685645
151.411894	4429.947416	24.690663
151.574834	4426.672510	24.695680
151.710838	4433.546245	24.700698
151.882600	4432.850270	24.705715
151.876071	4422.641761	24.710733
152.228480	4424.210186	24.715751
152.317470	4427.499395	24.720768
152.270078	4443.634160	24.725786
152.308183	4447.976209	24.730803
152.610689	4444.205464	24.735821
152.523263	4458.443626	24.740839
152.636231	4457.293662	24.745856
152.951863	4475.339678	24.750874
152.966991	4482.604810	24.755891
152.880450	4479.557681	24.760909
153.088047	4493.255592	24.765927
153.807081	4491.286829	24.770944
153.603369	4496.505267	24.775962
153.670274	4503.820371	24.780979
153.888991	4508.032163	24.785997
154.047513	4526.174088	24.791015
154.106465	4523.463276	24.796032
154.637187	4530.846848	24.801050
154.467257	4524.128916	24.806067
154.547848	4526.654820	24.811085
154.668694	4554.046439	24.816103
154.966639	4551.062302	24.821120
155.119377	4547.306752	24.826138
155.112051	4561.610915	24.831155
155.735314	4575.976629	24.836173
155.825155	4586.567855	24.841191
155.905456	4579.720325	24.846208
155.798445	4581.927638	24.851226
155.985967	4586.798957	24.856243
156.595257	4589.225645	24.861261
156.792663	4607.334725	24.866279
156.590449	4605.370412	24.871296
156.657321	4599.245629	24.876314
156.585157	4611.207950	24.881331
157.037432	4602.543630	24.886349
157.483032	4627.300102	24.891367
157.511494	4633.988893	24.896384
157.340259	4628.016126	24.901402
157.462237	4635.298915	24.906419
157.790945	4639.684379	24.911437
157.753468	4657.967063	24.916455
158.065219	4656.155249	24.921472
158.504686	4659.543621	24.926490
158.299889	4663.940975	24.931507
158.684058	4671.388103	24.936525
158.842904	4682.917160	24.941543
159.156544	4690.512426	24.946560
159.116491	4685.712152	24.951578
158.928323	4686.991521	24.956595
159.668322	4693.787978	24.961613
159.768616	4705.717378	24.966631
159.994264	4709.257066	24.971648
160.012670	4702.970825	24.976666
159.788860	4709.187720	24.981683
159.995479	4724.386247	24.986701
160.008001	4736.828434	24.991719
160.468723	4737.463117	24.996736
160.539172	4746.775221	25.001754
160.403245	4765.802220	25.006771
160.918891	4761.724433	25.011789
161.068072	4768.275248	25.016807
161.286940	4788.225170	25.021824
161.580125	4791.249832	25.026842
161.593963	4802.925612	25.031859
161.904768	4797.653990	25.036877
162.096991	4797.871253	25.041895
161.916031	4811.529914	25.046912
162.003340	4821.056509	25.051930
162.338176	4827.216657	25.056947
162.384207	4817.100982	25.061965
162.410003	4832.739107	25.066983
162.691791	4845.676573	25.072000
163.084729	4839.856880	25.077018
163.133159	4854.320795	25.082035
163.138366	4853.315426	25.087053
163.507888	4868.257628	25.092071
163.677653	4870.612034	25.097088
164.032479	4874.703110	25.102106
163.989751	4883.765860	25.107123
164.286696	4871.290921	25.112141
164.359240	4871.299903	25.117159
164.568201	4890.320862	25.122176
164.752546	4892.667442	25.127194
164.637166	4902.636277	25.132211
164.917840	4889.057011	25.137229
164.872715	4896.844102	25.142247
164.876937	4918.185497	25.147264
165.314883	4919.009485	25.152282
164.973800	4926.257666	25.157299
165.840382	4938.810911	25.162317
165.499406	4954.481669	25.167335
165.763757	4952.143196	25.172352
166.140476	4963.551992	25.177370
166.218610	4982.079411	25.182387
166.417282	4981.122653	25.187405
166.852855	4995.362930	25.192423
167.310820	5000.213306	25.197440
167.217467	5006.245892	25.202458
167.366710	5007.807433	25.207475
167.666331	5004.784391	25.212493
167.649732	5011.057281	25.217511
167.627988	5021.447113	25.222528
168.124225	5028.421049	25.227546
167.821881	5030.938064	25.232563
168.051721	5033.053985	25.237581
168.062800	5047.686896	25.242599
168.608337	5060.929453	25.247616
168.577841	5057.591624	25.252634
168.860070	5073.562821	25.257651
169.506780	5078.269848	25.262669
169.152859	5091.459130	25.267687
169.465357	5082.425025	25.272704
169.930283	5075.515956	25.277722
169.879037	5087.669649	25.282739
170.100363	5100.239351	25.287757
170.442546	5107.566732	25.292775
170.431435	5111.657990	25.297792
170.618761	5110.728208	25.302810
170.514709	5124.380406	25.307827
170.936724	5119.931166	25.312845
170.824731	5129.666743	25.317863
170.698248	5139.277187	25.322880
171.240137	5127.397091	25.327898
171.109166	5136.445739	25.332915
171.418860	5161.107554	25.337933
171.865206	5152.919831	25.342951
172.046382	5150.271242	25.347968
171.870642	5148.639353	25.352986
171.830750	5180.391051	25.358003
172.169524	5186.756847	25.363021
172.612725	5190.699395	25.368039
172.498828	5198.411068	25.373056
173.130651	5206.075467	25.378074
172.799948	5214.740608	25.383091
172.989097	5223.319741	25.388109
173.071369	5226.998059	25.393127
173.183754	5246.388115	25.398144
173.616523	5252.646910	25.403162
173.449650	5268.246189	25.408179
174.055029	5273.047984	25.413197
174.194078	5275.349135	25.418215
174.268762	5291.751739	25.423232
174.882239	5296.556971	25.428250
174.778333	5296.489445	25.433267
175.123541	5294.346516	25.438285
175.261873	5298.961571	25.443303
175.189955	5306.857785	25.448320
175.770192	5321.550509	25.453338
175.814339	5335.152529	25.458355
176.145524	5328.499110	25.463373
176.225761	5320.541949	25.468391
175.731868	5326.190072	25.473408
176.190657	5323.708833	25.478426
176.585983	5340.096571	25.483443
176.494301	5341.134035	25.488461
177.040965	5351.498793	25.493479
177.305368	5363.839994	25.498496
177.689336	5359.413271	25.503514
177.580789	5367.600942	25.508531
177.773045	5366.577523	25.513549
178.092348	5359.532615	25.518567
178.065522	5371.486752	25.523584
178.823823	5377.714953	25.528602
178.612585	5391.823483	25.533619
178.792609	5392.159926	25.538637
178.622645	5385.443964	25.543655
178.510421	5391.840829	25.548672
178.980833	5399.979502	25.553690
179.111931	5421.695558	25.558707
179.418224	5414.739239	25.563725
179.347490	5419.610305	25.568743
179.441283	5435.283075	25.573760
179.791321	5450.378458	25.578778
179.568285	5443.102114	25.583795
179.969709	5450.268384	25.588813
180.527813	5469.085745	25.593831
180.688248	5467.210628	25.598848
180.984143	5462.519406	25.603866
181.053611	5481.926055	25.608883
181.027699	5494.948545	25.613901
181.584059	5480.837799	25.618919
181.619048	5486.237249	25.623936
181.923395	5485.918188	25.628954
181.740244	5495.494624	25.633971
181.840211	5496.908298	25.638989
182.053300	5508.497017	25.644007
182.018105	5520.861716	25.649024
182.373490	5516.825009	25.654042
182.378262	5539.790273	25.659059
182.794927	5550.868234	25.664077
182.841155	5546.599928	25.669095
182.924068	5566.493115	25.674112
183.272967	5572.287860	25.679130
183.612166	5576.830075	25.684148
183.540047	5582.571560	25.689165
183.915945	5589.173148	25.694183
183.983656	5605.109883	25.699200
184.446874	5602.097624	25.704218
184.337581	5621.222182	25.709236
184.427889	5629.911719	25.714253
184.880859	5635.068366	25.719271
184.890772	5635.521620	25.724288
185.106249	5650.862095	25.729306
185.234971	5659.012107	25.734324
185.204970	5667.187423	25.739341
185.739730	5674.790441	25.744359
185.855567	5690.197192	25.749376
186.058106	5695.696680	25.754394
186.448055	5716.601675	25.759412
186.277776	5721.388003	25.764429
186.653866	5717.897099	25.769447
186.848948	5742.058896	25.774464
187.102282	5749.120677	25.779482
187.504841	5746.015780	25.784500
187.123912	5747.296065	25.789517
187.707849	5760.149199	25.794535
187.830360	5775.261514	25.799552
187.927708	5761.020685	25.804570
188.090323	5787.756502	25.809588
188.115949	5792.621772	25.814605
188.728083	5788.525186	25.819623
188.914843	5795.855659	25.824640
189.191693	5820.048609	25.829658
189.002665	5821.339224	25.834676
189.333575	5817.608455	25.839693
189.686581	5822.113929	25.844711
189.452586	5838.777983	25.849728
189.943079	5842.319005	25.854746
190.226139	5841.158347	25.859764
190.234074	5843.383715	25.864781
190.637613	5857.212953	25.869799
190.549796	5863.421240	25.874816
191.047126	5865.199612	25.879834
191.047951	5869.608603	25.884852
191.386980	5878.122531	25.889869
191.529137	5889.239782	25.894887
191.237723	5903.331681	25.899904
191.645071	5896.672164	25.904922
191.912967	5897.634256	25.909940
191.704430	5921.116400	25.914957
192.238328	5922.705633	25.919975
192.319007	5933.726504	25.924992
192.436169	5945.907559	25.930010
192.689117	5968.294206	25.935028
192.729551	5954.406869	25.940045
193.108319	5970.200005	25.945063
193.076435	5992.267814	25.950080
193.190824	5991.476276	25.955098
193.401229	6010.841485	25.960116
193.499643	6019.531532	25.965133
193.879801	6028.314362	25.970151
194.122470	6041.740624	25.975168
194.184718	6051.241324	25.980186
194.152089	6069.531275	25.985204
194.485628	6079.015502	25.990221
195.226486	6081.150047	25.995239
195.215573	6102.117910	26.000256
195.597454	6098.482016	26.005274
196.167106	6108.500615	26.010292
196.153781	6117.173125	26.015309
196.625525	6125.849362	26.020327
196.636392	6128.541653	26.025344
196.878362	6127.084614	26.030362
197.134473	6121.380650	26.035380
197.052942	6121.739919	26.040397
197.546595	6124.220717	26.045415
197.903703	6151.995425	26.050432
197.974085	6150.401297	26.055450
198.050159	6150.001380	26.060468
198.107167	6150.266971	26.065485
198.434749	6145.479220	26.070503
198.396832	6146.013285	26.075520
198.261541	6162.795722	26.080538
198.639939	6169.358622	26.085556
198.442720	6171.995181	26.090573
198.964603	6182.018297	26.095591
198.719902	6200.154171	26.100608
199.109435	6208.254261	26.105626
199.398757	6220.949409	26.110644
199.357600	6238.661855	26.115661
199.744530	6253.162093	26.120679
199.922026	6253.695658	26.125696
200.233147	6277.538497	26.130714
200.505461	6287.787147	26.135732
200.458987	6291.468157	26.140749
200.905277	6300.698520	26.145767
201.139647	6308.315918	26.150784
201.307878	6309.393846	26.155802
201.965176	6315.493787	26.160820
202.113400	6329.707204	26.165837
202.466152	6323.610888	26.170855
202.710636	6330.632660	26.175872
202.878775	6323.263633	26.180890
203.125577	6324.321171	26.185908
203.109393	6326.280587	26.190925
203.224438	6323.281197	26.195943
203.017501	6330.816310	26.200960
203.097180	6347.044623	26.205978
203.638102	6345.427403	26.210996
203.342999	6362.614771	26.216013
203.507812	6378.691073	26.221031
203.725091	6390.124821	26.226048
203.923597	6412.824522	26.231066
204.208433	6418.836742	26.236084
204.032542	6438.227103	26.241101
204.467856	6443.247591	26.246119
204.691195	6474.952241	26.251136
205.150612	6482.721904	26.256154
205.613597	6496.132347	26.261172
205.612870	6507.803927	26.266189
206.300937	6504.129363	26.271207
206.541668	6505.805520	26.276224
206.730837	6523.026037	26.281242
207.015780	6527.659812	26.286260
207.207793	6530.756043	26.291277
207.332907	6527.231785	26.296295
207.451271	6530.252419	26.301312
207.165326	6538.458782	26.306330
207.863543	6541.506591	26.311348
207.656716	6556.224507	26.316365
208.088417	6566.739063	26.321383
208.518956	6577.788838	26.326400
208.614378	6579.986997	26.331418
208.932012	6580.498239	26.336436
209.229154	6587.515675	26.341453
209.548785	6594.819074	26.346471
209.621310	6609.623914	26.351488
209.738325	6603.648459	26.356506
210.007830	6609.595536	26.361524
209.639215	6621.568178	26.366541
209.900707	6631.065819	26.371559
210.418080	6624.678777	26.376576
210.122600	6644.868192	26.381594
210.833200	6653.720685	26.386612
210.678665	6666.510566	26.391629
211.385800	6672.028346	26.396647
211.483228	6678.553643	26.401664
211.477913	6689.813810	26.406682
212.031462	6698.570980	26.411700
211.965327	6720.993889	26.416717
212.279215	6717.375767	26.421735
212.456267	6718.609682	26.426752
212.601264	6725.462600	26.431770
213.070568	6730.568253	26.436788
213.123248	6737.402844	26.441805
213.304313	6744.829902	26.446823
213.432437	6749.026096	26.451840
213.578786	6761.194517	26.456858
213.880778	6770.698382	26.461876
213.690925	6781.774018	26.466893
213.845141	6790.613775	26.471911
214.267837	6801.305394	26.476928
214.178902	6826.366351	26.481946
215.018094	6826.945544	26.486964
215.143020	6839.670575	26.491981
215.887556	6848.689304	26.496999
215.819655	6857.830446	26.502016
215.512248	6856.803954	26.507034
216.134678	6859.397330	26.512052
216.137414	6871.959323	26.517069
216.231987	6882.815814	26.522087
216.677312	6887.459548	26.527104
216.660268	6905.446693	26.532122
217.100754	6899.016712	26.537140
216.885192	6924.493787	26.542157
217.095932	6931.145124	26.547175
217.824853	6939.297748	26.552192
217.720802	6962.713739	26.557210
218.348799	6960.571145	26.562228
218.583699	6972.345590	26.567245
218.708772	6982.399454	26.572263
219.260942	6985.932505	26.577280
219.277192	6993.971354	26.582298
219.667519	6991.149053	26.587316
219.582943	7001.009739	26.592333
219.866454	7005.403125	26.597351
220.076980	7016.068132	26.602368
219.931397	7017.732746	26.607386
220.431811	7034.650107	26.612404
220.762564	7049.690405	26.617421
220.973667	7052.120408	26.622439
220.973694	7052.833362	26.627456
220.837106	7066.639668	26.632474
221.211326	7071.047730	26.637492
221.331559	7087.212951	26.642509
221.557512	7100.278537	26.647527
221.902730	7109.361072	26.652544
221.958721	7128.367595	26.657562
222.656416	7127.422445	26.662580
222.791045	7148.776170	26.667597
222.984923	7151.537044	26.672615
223.159019	7159.727863	26.677632
223.545799	7177.024655	26.682650
223.766588	7185.649460	26.687668
223.449570	7196.702396	26.692685
223.893800	7206.725215	26.697703
224.380498	7217.449426	26.702720
224.469421	7227.059147	26.707738
224.723433	7243.030112	26.712756
225.154886	7247.872882	26.717773
224.965565	7260.572822	26.722791
224.943862	7267.210213	26.727808
225.481131	7279.862821	26.732826
225.983389	7273.156885	26.737844
225.698770	7292.792297	26.742861
225.922705	7301.566955	26.747879
226.709810	7311.229905	26.752896
226.546261	7324.149648	26.757914
226.709300	7336.828115	26.762932
226.963366	7340.452042	26.767949
226.864128	7363.930844	26.772967
227.273914	7368.478106	26.777984
227.809756	7386.989880	26.783002
227.835587	7395.242228	26.788020
227.922870	7404.887733	26.793037
228.253631	7423.628950	26.798055
228.910683	7421.725588	26.803072
228.848824	7433.976529	26.808090
229.174498	7454.293078	26.813108
228.984651	7451.825968	26.818125
229.758894	7473.642389	26.823143
229.893140	7477.180009	26.828160
229.760766	7490.724801	26.833178
230.536328	7501.958698	26.838196
230.734257	7519.466178	26.843213
230.869618	7515.179956	26.848231
231.419708	7526.854249	26.853248
231.163488	7536.582126	26.858266
231.590617	7533.283323	26.863284
231.919930	7539.506086	26.868301
232.151830	7563.229070	26.873319
232.337660	7567.162146	26.878336
232.295701	7571.351848	26.883354
232.680730	7579.073363	26.888372
232.889163	7595.397401	26.893389
233.014537	7596.428751	26.898407
233.495965	7605.372642	26.903424
233.443275	7622.138836	26.908442
233.923539	7626.714291	26.913460
234.118486	7643.838406	26.918477
234.153094	7646.158937	26.923495
234.354917	7650.411313	26.928512
234.483140	7672.902249	26.933530
235.093027	7668.868476	26.938548
234.933028	7696.032123	26.943565
235.166030	7707.049707	26.948583
235.480712	7717.044736	26.953600
235.536544	7739.985593	26.958618
236.014377	7738.435733	26.963636
236.309782	7766.595490	26.968653
236.604025	7765.833426	26.973671
236.631126	7783.212643	26.978688
236.894268	7793.980772	26.983706
237.596482	7796.132765	26.988724
237.997791	7796.394661	26.993741
237.973345	7808.413329	26.998759
238.206286	7815.849181	27.003776
238.241025	7819.201304	27.008794
238.608794	7822.416942	27.013812
238.646646	7827.189655	27.018829
239.045788	7844.242114	27.023847
239.141413	7838.804647	27.028864
239.112901	7854.530156	27.033882
239.752329	7862.231734	27.038900
239.746818	7863.972475	27.043917
239.975749	7884.853481	27.048935
240.146069	7892.665248	27.053952
240.086674	7906.086262	27.058970
240.624264	7918.352227	27.063988
240.460212	7936.919579	27.069005
240.912054	7950.230828	27.074023
241.295197	7966.986966	27.079040
241.167801	7985.246375	27.084058
241.713560	7990.051503	27.089076
242.146007	8000.843947	27.094093
242.167853	8022.505684	27.099111
242.604939	8028.725642	27.104128
242.942198	8046.274488	27.109146
243.280499	8047.518229	27.114164
243.465365	8068.892808	27.119181
243.868593	8068.731850	27.124199
244.215232	8070.846917	27.129216
244.287089	8080.562204	27.134234
244.443881	8091.696088	27.139252
244.856887	8092.680060	27.144269
244.791972	8102.188176	27.149287
245.039496	8119.461836	27.154304
245.125214	8132.725370	27.159322
245.420524	8147.562333	27.164340
245.713727	8158.226789	27.169357
245.845815	8178.563378	27.174375
246.328762	8182.828547	27.179392
246.385328	8205.893938	27.184410
246.608563	8219.468094	27.189428
247.013313	8228.062614	27.194445
246.929655	8251.237375	27.199463
247.352253	8253.658267	27.204480
247.500639	8271.398792	27.209498
248.137606	8275.528883	27.214516
248.753959	8288.803596	27.219533
248.871512	8300.480157	27.224551
249.693698	8286.669469	27.229568
249.582910	8296.939650	27.234586
249.815634	8283.869340	27.239604
249.960475	8300.848359	27.244621
249.732152	8313.670294	27.249639
250.100554	8320.887302	27.254656
250.333314	8327.404740	27.259674
250.846740	8349.345859	27.264692
250.620680	8345.233068	27.269709
251.097588	8353.764227	27.274727
251.350550	8365.274864	27.279744
251.653616	8378.202202	27.284762
251.629338	8378.917126	27.289780
252.056193	8388.415511	27.294797
252.142798	8410.163098	27.299815
252.406160	8410.827853	27.304832
252.623222	8421.496764	27.309850
252.623895	8437.190693	27.314868
253.047315	8443.305593	27.319885
253.131734	8464.682977	27.324903
253.158492	8466.633077	27.329920
253.648834	8487.968623	27.334938
253.980032	8511.065081	27.339956
254.539691	8521.899798	27.344973
254.398705	8537.410239	27.349991
254.616638	8555.357204	27.355008
254.911306	8561.382112	27.360026
255.745128	8592.604468	27.365044
255.821492	8591.819645	27.370061
255.751108	8614.517559	27.375079
256.048827	8619.605582	27.380096
256.073214	8638.651723	27.385114
256.278596	8655.979542	27.390132
256.747344	8669.542917	27.395149
256.815383	8689.965166	27.400167
257.608480	8700.666022	27.405184
257.764499	8721.590903	27.410202
258.145986	8732.343607	27.415220
258.291760	8745.469848	27.420237
258.419554	8753.920345	27.425255
258.839194	8764.563906	27.430272
258.952327	8784.181556	27.435290
259.310919	8800.167824	27.440308
259.603521	8806.883291	27.445325
259.695723	8828.754534	27.450343
260.033564	8834.446101	27.455360
260.262471	8841.920096	27.460378
260.662804	8872.005770	27.465396
260.956192	8875.080833	27.470413
261.158211	8893.834977	27.475431
261.552499	8904.849780	27.480448
261.742932	8904.331629	27.485466
262.074060	8925.112031	27.490484
262.151456	8925.224910	27.495501
262.205674	8934.675615	27.500519
262.701391	8954.061754	27.505536
262.962460	8963.145462	27.510554
263.074404	8979.660306	27.515572
263.332373	8993.442495	27.520589
262.927053	9022.743632	27.525607
263.408687	9025.414541	27.530624
263.969742	9051.386065	27.535642
264.101276	9065.229390	27.540660
264.460489	9075.386642	27.545677
264.750043	9084.284103	27.550695
264.988078	9108.632606	27.555712
265.113875	9121.348432	27.560730
265.279273	9140.355819	27.565748
266.300548	9152.839648	27.570765
266.221938	9178.172822	27.575783
266.706649	9176.200718	27.580800
266.669653	9186.360199	27.585818
267.072203	9206.982453	27.590836
267.081218	9213.722836	27.595853
267.507579	9227.732589	27.600871
267.824358	9239.586675	27.605888
268.447245	9249.248747	27.610906
268.682161	9272.195287	27.615924
268.862804	9266.883832	27.620941
268.881408	9281.193519	27.625959
269.496446	9284.339780	27.630976
269.442461	9299.370090	27.635994
269.406552	9322.614837	27.641012
270.289742	9316.017280	27.646029
270.229593	9342.841023	27.651047
270.544550	9351.328923	27.656064
270.843701	9367.806098	27.661082
271.060047	9395.571526	27.666100
271.613643	9397.295352	27.671117
271.413120	9415.819193	27.676135
271.645345	9418.299345	27.681152
272.172646	9436.539998	27.686170
272.216930	9448.773704	27.691188
272.701200	9465.921089	27.696205
272.873558	9482.992286	27.701223
272.760803	9502.353340	27.706240
273.540738	9514.734677	27.711258
273.283087	9530.188792	27.716276
274.115040	9547.245057	27.721293
274.129302	9560.769530	27.726311
274.563761	9580.962650	27.731328
274.876382	9596.689924	27.736346
274.702293	9626.719919	27.741364
274.787948	9632.747880	27.746381
275.701521	9652.610556	27.751399
275.761577	9669.187942	27.756416
276.102533	9688.643375	27.761434
276.196954	9708.400575	27.766452
276.676664	9720.202715	27.771469
276.761514	9747.096540	27.776487
277.161476	9763.095346	27.781504
277.301837	9782.003657	27.786522
277.464731	9807.286420	27.791540
278.103559	9817.424410	27.796557
278.366904	9837.843462	27.801575
278.551497	9854.807678	27.806592
279.165155	9855.206167	27.811610
279.213722	9872.004780	27.816628
279.707598	9886.916105	27.821645
279.680629	9901.524826	27.826663
279.703027	9908.862672	27.831680
280.352049	9921.988839	27.836698
280.392502	9940.032247	27.841716
280.546258	9943.561837	27.846733
280.777292	9969.972776	27.851751
281.094620	9983.504028	27.856768
281.090403	9998.016353	27.861786
281.293990	10025.498125	27.866804
282.198796	10041.527744	27.871821
282.076177	10061.089407	27.876839
282.109232	10082.977019	27.881856
282.862768	10103.522934	27.886874
282.912919	10128.974519	27.891892
283.564569	10132.004953	27.896909
283.691758	10175.793412	27.901927
284.091137	10186.572254	27.906944
284.589073	10205.185656	27.911962
284.569226	10220.052866	27.916980
285.024760	10236.610746	27.921997
285.116823	10253.814845	27.927015
285.423965	10274.202327	27.932032
285.848780	10280.828529	27.937050
286.114648	10303.589917	27.942068
286.413273	10318.469040	27.947085
286.761722	10338.895280	27.952103
287.203801	10348.839904	27.957120
287.432420	10362.966442	27.962138
287.410825	10382.938585	27.967156
287.892663	10403.861506	27.972173
288.238707	10411.975557	27.977191
288.425581	10434.102420	27.982208
288.801490	10449.767775	27.987226
288.777290	10465.090415	27.992244
289.219623	10478.344843	27.997261
289.445353	10501.767325	28.002279
290.011353	10513.062493	28.007296
290.152023	10521.702786	28.012314
290.380284	10563.395410	28.017332
290.679481	10563.915654	28.022349
291.096190	10576.711489	28.027367
291.257105	10596.429352	28.032384
291.827891	10611.536326	28.037402
291.983706	10621.791578	28.042420
292.405747	10643.705770	28.047437
292.660301	10657.846161	28.052455
292.767634	10682.620997	28.057472
293.512549	10685.630392	28.062490
293.479912	10726.014515	28.067508
293.662696	10728.565335	28.072525
294.054718	10741.943705	28.077543
293.973887	10763.255464	28.082560
294.350111	10789.520354	28.087578
294.284949	10810.421216	28.092596
294.513411	10824.808325	28.097613
294.948245	10839.632417	28.102631
295.126738	10860.967132	28.107648
295.791187	10869.260900	28.112666
295.863158	10898.501421	28.117684
296.470864	10912.958829	28.122701
296.802122	10926.322256	28.127719
296.882453	10940.441485	28.132736
297.461489	10956.595622	28.137754
297.427663	10975.449762	28.142772
297.933756	10992.839399	28.147789
298.062900	11007.905980	28.152807
298.603878	11033.841641	28.157824
299.050192	11036.206099	28.162842
298.969199	11065.126595	28.167860
299.353370	11074.463892	28.172877
299.862982	11091.443822	28.177895
299.809184	11108.632393	28.182912
300.459873	11135.356677	28.187930
300.613176	11154.346894	28.192948
300.855355	11163.932360	28.197965
301.424661	11188.716265	28.202983
301.939688	11199.961442	28.208000
302.000166	11220.835373	28.213018
302.158315	11233.714684	28.218036
302.423363	11255.319108	28.223053
302.739893	11268.917759	28.228071
302.586331	11289.900268	28.233088
303.098101	11308.543530	28.238106
303.643103	11334.556200	28.243124
303.684643	11350.969168	28.248141
304.140926	11373.868686	28.253159
304.763273	11399.361492	28.258176
304.997194	11411.647640	28.263194
305.439555	11439.685021	28.268212
305.761651	11454.686671	28.273229
306.048912	11463.523735	28.278247
305.977592	11482.695173	28.283264
306.447467	11497.294938	28.288282
306.712621	11521.210536	28.293300
307.022603	11526.325936	28.298317
307.589315	11550.172277	28.303335
307.701409	11560.387518	28.308352
308.139280	11587.875338	28.313370
308.158993	11600.520438	28.318388
308.875092	11614.169462	28.323405
309.285388	11628.180480	28.328423
309.379560	11654.500479	28.333440
309.513172	11662.818279	28.338458
309.923940	11678.573415	28.343476
310.407472	11699.521087	28.348493
310.475758	11711.028305	28.353511
310.612869	11731.239427	28.358528
311.321804	11742.255771	28.363546
311.296854	11757.484997	28.368564
311.481415	11770.892619	28.373581
312.199644	11787.484533	28.378599
312.363763	11802.391869	28.383616
312.651408	11815.583976	28.388634
312.624694	11826.115684	28.393652
312.869109	11842.173959	28.398669
313.235306	11861.616179	28.403687
313.253457	11883.998927	28.408704
313.908564	11902.909142	28.413722
314.275617	11934.568803	28.418740
314.439359	11954.964486	28.423757
314.904036	11966.436284	28.428775
314.804481	11997.679482	28.433792
315.217757	12007.205558	28.438810
315.565032	12024.625434	28.443828
316.083824	12052.360944	28.448845
316.771296	12068.926587	28.453863
316.863939	12088.977228	28.458880
317.428015	12099.692636	28.463898
317.607038	12120.277371	28.468916
317.635416	12140.674999	28.473933
318.046358	12157.436318	28.478951
318.315838	12184.660830	28.483968
318.773086	12201.269599	28.488986
318.919838	12221.626042	28.494004
319.056586	12237.489967	28.499021
319.910000	12260.569388	28.504039
320.028855	12288.807670	28.509056
320.563283	12297.795926	28.514074
320.967709	12324.444083	28.519092
321.661136	12324.659152	28.524109
321.980968	12335.786340	28.529127
322.279092	12357.698172	28.534144
322.487728	12354.306048	28.539162
323.000144	12372.096319	28.544180
322.946064	12377.418389	28.549197
323.668557	12398.704800	28.554215
323.466522	12407.123718	28.559232
324.138764	12422.261609	28.564250
324.280358	12439.390250	28.569268
324.487280	12454.565518	28.574285
324.829278	12462.825368	28.579303
324.925311	12486.347350	28.584320
325.052355	12502.187320	28.589338
325.362774	12522.676495	28.594356
325.682822	12538.405268	28.599373
326.019204	12561.320970	28.604391
326.530855	12587.661863	28.609408
326.448246	12603.044969	28.614426
327.120875	12629.904381	28.619444
327.511162	12657.128990	28.624461
328.152853	12665.775886	28.629479
328.032362	12693.109297	28.634496
328.668490	12711.416680	28.639514
328.914485	12726.359106	28.644532
329.366382	12741.309080	28.649549
329.695388	12756.991786	28.654567
329.749169	12769.615114	28.659584
330.214618	12781.231455	28.664602
330.595244	12805.914268	28.669620
330.605806	12821.377402	28.674637
331.479065	12826.791946	28.679655
331.364097	12849.438581	28.684672
331.716780	12861.191415	28.689690
331.947934	12886.347234	28.694708
332.177818	12887.632293	28.699725
332.788440	12912.681449	28.704743
332.933589	12933.038118	28.709760
333.484724	12948.732858	28.714778
334.062898	12965.224415	28.719796
334.386448	12987.963536	28.724813
335.003090	12979.342248	28.729831
334.809709	13006.559138	28.734848
334.938797	13020.545610	28.739866
335.207871	13033.703956	28.744884
335.258348	13059.935354	28.749901
335.960145	13075.838427	28.754919
336.200141	13110.948204	28.759936
336.524947	13121.967341	28.764954
336.830995	13142.983962	28.769972
336.859310	13170.858707	28.774989
337.627665	13194.024446	28.780007
337.967376	13221.773413	28.785024
338.165649	13231.664929	28.790042
338.828462	13266.124220	28.795060
338.923616	13282.398295	28.800077
339.559687	13297.192053	28.805095
339.428306	13322.586812	28.810112
340.027603	13346.424795	28.815130
340.573769	13364.781938	28.820148
340.803968	13390.181876	28.825165
341.165291	13404.854409	28.830183
341.588707	13433.543971	28.835200
341.861947	13442.869912	28.840218
342.217061	13476.780169	28.845236
342.464914	13486.493825	28.850253
342.978722	13502.302560	28.855271
343.123655	13520.548283	28.860288
343.664430	13534.809886	28.865306
344.420713	13551.763814	28.870324
344.581717	13565.316991	28.875341
345.159458	13580.087161	28.880359
345.527120	13585.173609	28.885376
345.853543	13604.835365	28.890394
346.221448	13614.469462	28.895412
346.148496	13622.576538	28.900429
346.482020	13635.166835	28.905447
346.428063	13662.402333	28.910464
346.672583	13683.320382	28.915482
347.572906	13695.807632	28.920500
347.572638	13717.858509	28.925517
347.964088	13733.592692	28.930535
348.094607	13744.205763	28.935552
348.332524	13771.448478	28.940570
348.761950	13791.071334	28.945588
348.809455	13811.989168	28.950605
349.515329	13830.431045	28.955623
349.609744	13844.154287	28.960640
350.267773	13871.213545	28.965658
350.674402	13892.219210	28.970676
350.717951	13920.360932	28.975693
351.019549	13939.575134	28.980711
351.234996	13975.073877	28.985728
351.882855	13988.072529	28.990746
352.174595	14007.486955	28.995764
352.573447	14029.228497	29.000781
353.375251	14046.088349	29.005799
353.510503	14072.881056	29.010816
353.517220	14091.719412	29.015834
354.322797	14107.786420	29.020852
354.141989	14139.254572	29.025869
354.892221	14153.186810	29.030887
355.005009	14177.163437	29.035904
355.533895	14207.060370	29.040922
355.971660	14231.286409	29.045940
356.282516	14257.379486	29.050957
356.618431	14272.532081	29.055975
356.821160	14300.288503	29.060992
357.552875	14323.874574	29.066010
358.151193	14327.215301	29.071028
358.313970	14357.767956	29.076045
358.443249	14376.420345	29.081063
358.695344	14400.641106	29.086080
359.155300	14426.889217	29.091098
359.619664	14441.547023	29.096116
359.518079	14472.141435	29.101133
360.235231	14494.473229	29.106151
360.625676	14508.106999	29.111168
360.611348	14534.263674	29.116186
361.217000	14556.001753	29.121204
361.785318	14582.708741	29.126221
361.780338	14594.702143	29.131239
362.061999	14623.280832	29.136256
362.656882	14652.744499	29.141274
363.175536	14677.309854	29.146292
363.597340	14703.645899	29.151309
364.092423	14717.243505	29.156327
364.256684	14743.104819	29.161344
364.277347	14770.303827	29.166362
364.879429	14791.333615	29.171380
365.335722	14818.253211	29.176397
365.675647	14838.425911	29.181415
366.157393	14858.730044	29.186432
366.731765	14876.299353	29.191450
367.265221	14891.979143	29.196468
367.193652	14906.573994	29.201485
367.322389	14918.690705	29.206503
368.001222	14943.861055	29.211520
368.230613	14965.654449	29.216538
368.607956	14979.520307	29.221556
368.992891	14997.857385	29.226573
369.268593	15025.661259	29.231591
369.646601	15037.296018	29.236608
369.716396	15063.775164	29.241626
370.296403	15072.832409	29.246644
370.420276	15100.924926	29.251661
370.874709	15118.406656	29.256679
371.262670	15154.285785	29.261696
371.649937	15176.475308	29.266714
372.338811	15193.839572	29.271732
372.811460	15221.822424	29.276749
373.061100	15241.208812	29.281767
373.409754	15261.705815	29.286784
373.801021	15283.987654	29.291802
374.330435	15299.692715	29.296820
374.228200	15325.114289	29.301837
374.531522	15347.950095	29.306855
375.072534	15369.433931	29.311872
375.678913	15391.406115	29.316890
375.973461	15417.711310	29.321908
376.074663	15437.158890	29.326925
376.399753	15460.194706	29.331943
377.295845	15485.560627	29.336960
377.603639	15516.378066	29.341978
377.837344	15529.205775	29.346996
378.035659	15563.707947	29.352013
378.476475	15578.519196	29.357031
378.883221	15598.261848	29.362048
378.957803	15623.641574	29.367066
379.451332	15649.515924	29.372084
380.087387	15681.851618	29.377101
380.534719	15702.775152	29.382119
381.024237	15733.508769	29.387136
381.224426	15759.036791	29.392154
381.839723	15782.288430	29.397172
382.077336	15813.783293	29.402189
382.312689	15829.042219	29.407207
382.809789	15856.900699	29.412224
382.873858	15887.153666	29.417242
383.216494	15905.751977	29.422260
383.867882	15930.860224	29.427277
384.320046	15955.542639	29.432295
384.989121	15983.351907	29.437312
385.107162	16005.560425	29.442330
385.761217	16024.185045	29.447348
385.909811	16045.569771	29.452365
386.201276	16067.982609	29.457383
387.004763	16085.079761	29.462400
387.168439	16111.876419	29.467418
387.766692	16105.700703	29.472436
388.354564	16126.314864	29.477453
388.564394	16137.255301	29.482471
389.042838	16149.180969	29.487488
389.088473	16169.276139	29.492506
389.597005	16176.168543	29.497524
389.943195	16205.386370	29.502541
390.089586	16210.453647	29.507559
390.389324	16237.553020	29.512576
390.648075	16260.395315	29.517594
391.203538	16282.210570	29.522612
391.160702	16313.468490	29.527629
391.734469	16333.359673	29.532647
392.236585	16357.363988	29.537664
392.589146	16394.142691	29.542682
393.052646	16421.360967	29.547700
393.291934	16450.353206	29.552717
393.357971	16471.492255	29.557735
394.267520	16498.774240	29.562752
394.165414	16532.583508	29.567770
394.401339	16560.529748	29.572788
395.065201	16591.405202	29.577805
395.638723	16610.467929	29.582823
396.249954	16642.446644	29.587840
396.397967	16673.333582	29.592858
397.126851	16684.358829	29.597876
397.651277	16713.918876	29.602893
397.911563	16736.917130	29.607911
398.623332	16751.765869	29.612928
398.927103	16775.243823	29.617946
399.332285	16806.063092	29.622964
399.694007	16822.848802	29.627981
399.962979	16841.297002	29.632999
400.784264	16872.116449	29.638016
400.625619	16896.955746	29.643034
401.240469	16911.199658	29.648052
401.367066	16945.049764	29.653069
401.711620	16969.423415	29.658087
402.046114	16994.293356	29.663104
402.782890	17026.593395	29.668122
403.086014	17053.526941	29.673140
403.454221	17077.710985	29.678157
403.802255	17104.194976	29.683175
404.193689	17130.059540	29.688192
404.744147	17168.153158	29.693210
404.998371	17175.781170	29.698228
405.368028	17200.235039	29.703245
405.439472	17232.857235	29.708263
406.126343	17259.686507	29.713280
406.277413	17292.107571	29.718298
407.050626	17319.628272	29.723316
407.521097	17364.636130	29.728333
407.891140	17381.142987	29.733351
408.798961	17398.915308	29.738368
408.676953	17423.536433	29.743386
409.407587	17443.079077	29.748404
409.802812	17465.686857	29.753421
410.192915	17481.307200	29.758439
410.958082	17475.580128	29.763456
411.174916	17512.838608	29.768474
411.652369	17510.420611	29.773492
412.223050	17528.985737	29.778509
412.343830	17542.173553	29.783527
412.613605	17564.362896	29.788544
412.848471	17591.513167	29.793562
413.368751	17609.021496	29.798580
413.769451	17634.413201	29.803597
413.868032	17651.738764	29.808615
414.505713	17674.507826	29.813632
414.912481	17699.315618	29.818650
415.418684	17716.042082	29.823668
415.597628	17746.808915	29.828685
415.821734	17780.438626	29.833703
416.300589	17804.192213	29.838720
416.159407	17822.211264	29.843738
416.791853	17859.075635	29.848756
417.249799	17897.308029	29.853773
417.787942	17936.943864	29.858791
418.158956	17960.629438	29.863808
418.343014	17991.030196	29.868826
419.044537	18032.644167	29.873844
419.379395	18065.639929	29.878861
419.531929	18106.932892	29.883879
420.471848	18135.198964	29.888896
420.685747	18170.787444	29.893914
421.302291	18199.822470	29.898932
421.998395	18236.151612	29.903949
422.094904	18262.775094	29.908967
422.908498	18288.262729	29.913984
423.035728	18316.276697	29.919002
423.301798	18341.659511	29.924020
423.975503	18361.545858	29.929037
424.115665	18404.386485	29.934055
425.040878	18416.882719	29.939072
425.328103	18450.782177	29.944090
425.705578	18477.006932	29.949108
426.330905	18500.148478	29.954125
426.274366	18533.724128	29.959143
426.975970	18560.532446	29.964160
427.545883	18588.974433	29.969178
427.967051	18623.991154	29.974196
428.237882	18649.552064	29.979213
428.404993	18672.466061	29.984231
429.109873	18710.310321	29.989248
429.223112	18730.033656	29.994266
429.688698	18766.596043	29.999284
430.601016	18797.462315	30.004301
430.823314	18828.958272	30.009319
430.913969	18847.254581	30.014336
431.763356	18882.519828	30.019354
431.996875	18901.934443	30.024372
432.643400	18931.113708	30.029389
432.732182	18951.020362	30.034407
433.718079	18971.238886	30.039424
434.023105	19002.785011	30.044442
434.172588	19018.002297	30.049460
434.671524	19040.941936	30.054477
434.955003	19074.406710	30.059495
435.720420	19099.259616	30.064512
435.793234	19126.154505	30.069530
436.337425	19144.460421	30.074548
436.821253	19168.175933	30.079565
437.032402	19204.290475	30.084583
437.699142	19232.384336	30.089600
438.060020	19256.770400	30.094618
438.414396	19287.320194	30.099636
439.031178	19311.213579	30.104653
439.209263	19347.028184	30.109671
439.676782	19369.657541	30.114688
439.886558	19399.254526	30.119706
440.715638	19443.252937	30.124724
441.264996	19462.368708	30.129741
441.520011	19497.186674	30.134759
442.107717	19523.361199	30.139776
442.459461	19546.853818	30.144794
442.565525	19583.614773	30.149812
443.218770	19612.532805	30.154829
443.502683	19646.601155	30.159847
444.107445	19673.993412	30.164864
444.397569	19713.406718	30.169882
445.126704	19745.376209	30.174900
445.589317	19775.471090	30.179917
445.834401	19813.058559	30.184935
446.539339	19833.754901	30.189952
446.998780	19871.124094	30.194970
447.270681	19904.966549	30.199988
447.882997	19925.858102	30.205005
448.098142	19955.949830	30.210023
448.621103	19990.521466	30.215040
448.525754	20021.420347	30.220058
449.240357	20058.233533	30.225076
450.051663	20092.375560	30.230093
450.246144	20135.341038	30.235111
451.044129	20158.940292	30.240128
451.272372	20195.013449	30.245146
451.581217	20225.760543	30.250164
452.505315	20253.778634	30.255181
452.555770	20294.897552	30.260199
453.227875	20322.368422	30.265216
453.840440	20351.534102	30.270234
454.233057	20393.066559	30.275252
454.841245	20425.183104	30.280269
455.053131	20460.232555	30.285287
455.412823	20482.805099	30.290304
455.961113	20497.490940	30.295322
456.179341	20535.228930	30.300340
456.733292	20553.637326	30.305357
456.939373	20595.027563	30.310375
457.564367	20627.521433	30.315392
457.922229	20649.190822	30.320410
458.307237	20682.599550	30.325428
458.872382	20706.193800	30.330445
459.138633	20744.949222	30.335463
459.647643	20773.682501	30.340480
459.921156	20810.044399	30.345498
460.426143	20858.403088	30.350516
460.969074	20884.930788	30.355533
461.512559	20924.147306	30.360551
461.900880	20948.865556	30.365568
462.037030	20999.092413	30.370586
462.769369	21039.892032	30.375604
463.421693	21062.991742	30.380621
463.636917	21101.614411	30.385639
464.068570	21141.840811	30.390656
464.881951	21170.528701	30.395674
465.275520	21218.051748	30.400692
465.945457	21241.536395	30.405709
466.304382	21280.075184	30.410727
466.982988	21315.024638	30.415744
467.547684	21350.427047	30.420762
467.830449	21377.716851	30.425780
468.302299	21400.098407	30.430797
468.572875	21438.483117	30.435815
469.213006	21472.725514	30.440832
469.933950	21501.343676	30.445850
470.024912	21536.438412	30.450868
470.904279	21563.579960	30.455885
471.436054	21586.175906	30.460903
471.526792	21627.761284	30.465920
472.065742	21656.706421	30.470938
472.452183	21691.703247	30.475956
473.114826	21725.067608	30.480973
473.396251	21763.018211	30.485991
473.665260	21784.120507	30.491008
474.429654	21823.184370	30.496026
474.843563	21863.302028	30.501044
475.544643	21891.324710	30.506061
476.063880	21926.801028	30.511079
476.274227	21951.946148	30.516096
476.766770	21992.211491	30.521114
477.344220	22032.950935	30.526132
478.271283	22049.389380	30.531149
478.384864	22088.345694	30.536167
478.901471	22124.136340	30.541184
479.349280	22143.657490	30.546202
479.828524	22183.187455	30.551220
480.433413	22206.969808	30.556237
480.667169	22248.307210	30.561255
481.248523	22264.713519	30.566272
481.585532	22305.786529	30.571290
481.944419	22333.389572	30.576308
482.816032	22360.107635	30.581325
482.811587	22399.586011	30.586343
483.142411	22429.131223	30.591360
483.693724	22451.719789	30.596378
483.883360	22494.738549	30.601396
484.359206	22525.917209	30.606413
484.880039	22556.573660	30.611431
485.462684	22590.730768	30.616448
485.841776	22634.469552	30.621466
486.209669	22671.810757	30.626484
487.141559	22703.171537	30.631501
487.548347	22745.537316	30.636519
487.992759	22776.401698	30.641536
488.754938	22802.970964	30.646554
489.046892	22844.701561	30.651572
489.492087	22869.469690	30.656589
489.788648	22916.521815	30.661607
490.591850	22952.282081	30.666624
491.119364	22993.762890	30.671642
491.116678	23037.956627	30.676660
491.815573	23073.120991	30.681677
492.313420	23112.825963	30.686695
492.418499	23156.079739	30.691712
493.307237	23192.631120	30.696730
493.895637	23239.037528	30.701748
494.142426	23279.119231	30.706765
494.503177	23326.092245	30.711783
495.258566	23365.469336	30.716800
496.157271	23402.938031	30.721818
496.624567	23439.765047	30.726836
497.432732	23454.543812	30.731853
497.836476	23495.426539	30.736871
498.210362	23539.733408	30.741888
499.080241	23560.645496	30.746906
499.651328	23591.509408	30.751924
500.260802	23622.022265	30.756941
500.198144	23663.612998	30.761959
500.922937	23698.973910	30.766976
501.687964	23717.658019	30.771994
501.853209	23760.781767	30.777012
502.403508	23791.184647	30.782029
503.042185	23813.140551	30.787047
503.418218	23850.528922	30.792064
503.729664	23868.934927	30.797082
504.340371	23911.139011	30.802100
504.849252	23934.205130	30.807117
505.143423	23966.489971	30.812135
505.741408	24002.151386	30.817152
506.535321	24033.693535	30.822170
506.654265	24079.332757	30.827188
507.463934	24107.921828	30.832205
508.037071	24141.889234	30.837223
508.287244	24180.580015	30.842240
508.897942	24211.762572	30.847258
509.151241	24246.950094	30.852276
509.745296	24276.296921	30.857293
509.946923	24311.055636	30.862311
510.092207	24338.933290	30.867328
510.654816	24381.491300	30.872346
510.926429	24422.146172	30.877364
511.531556	24470.402281	30.882381
511.881216	24505.969674	30.887399
512.552197	24541.786883	30.892416
513.460502	24574.741603	30.897434
513.851187	24630.573220	30.902452
514.217823	24666.262728	30.907469
514.643986	24720.006256	30.912487
515.287631	24755.442312	30.917504
516.044001	24791.067668	30.922522
516.408379	24832.647790	30.927540
516.997871	24870.192827	30.932557
517.907801	24906.885003	30.937575
518.007061	24955.308218	30.942592
518.640620	24990.060279	30.947610
519.223146	25030.794801	30.952628
519.831771	25068.893407	30.957645
520.281185	25107.120654	30.962663
520.879301	25140.237806	30.967680
521.713857	25169.393581	30.972698
521.833179	25213.258025	30.977716
522.167653	25244.819027	30.982733
523.051243	25282.114957	30.987751
523.153718	25331.825206	30.992768
523.703793	25363.943716	30.997786
524.462095	25412.712384	31.002804
525.242318	25461.490313	31.007821
525.664455	25495.561065	31.012839
525.760176	25534.596404	31.017856
526.579821	25566.712568	31.022874
526.847970	25617.593944	31.027892
527.820764	25660.024654	31.032909
528.329252	25696.136601	31.037927
528.596532	25742.190222	31.042944
529.436623	25788.873574	31.047962
529.693545	25828.481883	31.052980
530.438403	25873.073325	31.057997
530.754216	25902.190943	31.063015
531.382221	25952.839610	31.068032
531.997822	25993.993573	31.073050
532.425703	26034.161282	31.078068
532.942600	26069.864655	31.083085
533.680391	26114.121504	31.088103
533.743877	26150.339216	31.093120
534.744861	26180.897042	31.098138
535.614805	26209.477926	31.103156
536.236229	26240.610746	31.108173
536.843884	26281.539038	31.113191
537.522825	26317.804863	31.118208
537.992986	26335.772477	31.123226
538.109851	26364.934434	31.128244
538.501988	26397.777382	31.133261
539.396057	26421.833552	31.138279
539.621722	26458.392465	31.143296
539.990520	26489.697565	31.148314
540.299477	26521.858371	31.153332
541.248147	26554.249042	31.158349
541.703661	26584.587255	31.163367
541.927901	26622.081123	31.168384
542.804947	26655.972391	31.173402
543.310625	26696.437408	31.178420
543.400949	26733.833112	31.183437
544.542979	26763.652668	31.188455
544.742582	26800.343349	31.193472
545.083405	26842.069517	31.198490
545.196631	26885.369892	31.203508
546.004442	26925.767676	31.208525
546.359450	26975.535757	31.213543
547.098109	27018.600597	31.218560
547.494173	27065.224441	31.223578
547.932811	27123.630199	31.228596
548.453203	27159.059690	31.233613
549.376548	27208.998766	31.238631
549.617471	27264.303231	31.243648
550.699887	27305.787237	31.248666
551.287891	27353.221204	31.253684
551.373764	27401.064596	31.258701
552.035729	27436.105009	31.263719
552.567617	27484.904998	31.268736
553.383131	27530.932373	31.273754
553.942030	27572.035589	31.278772
553.928002	27628.516431	31.283789
554.817928	27668.862823	31.288807
555.449728	27723.796195	31.293824
556.391498	27763.126085	31.298842
556.988583	27825.145209	31.303860
557.452002	27853.440789	31.308877
557.976645	27903.409263	31.313895
558.528461	27936.820048	31.318912
559.130084	27978.443804	31.323930
559.803024	28016.608499	31.328948
560.314424	28064.509003	31.333965
560.789774	28106.739389	31.338983
561.427612	28158.724973	31.344000
562.139242	28193.661424	31.349018
562.506587	28232.195178	31.354036
562.965089	28277.816671	31.359053
563.810416	28326.769418	31.364071
563.728618	28367.803341	31.369088
564.459104	28417.258424	31.374106
565.115450	28454.768103	31.379124
565.489419	28507.892024	31.384141
566.364617	28541.145407	31.389159
567.135936	28593.977841	31.394176
567.890002	28633.579270	31.399194
568.384233	28668.166859	31.404212
568.765554	28697.860581	31.409229
569.487141	28726.389201	31.414247
569.765781	28770.146547	31.419264
570.460498	28795.094496	31.424282
570.908099	28832.666656	31.429300
571.091973	28882.184984	31.434317
571.916328	28921.158185	31.439335
572.217891	28973.264539	31.444352
572.618880	29017.478982	31.449370
573.203590	29065.145418	31.454388
573.829332	29110.945912	31.459405
574.909268	29149.125690	31.464423
575.215144	29203.323302	31.469440
575.785410	29237.205026	31.474458
576.576160	29280.376337	31.479476
576.713350	29334.188358	31.484493
577.416151	29382.635908	31.489511
578.040773	29430.167834	31.494528
578.546289	29471.104715	31.499546
578.975747	29532.520384	31.504564
579.421380	29581.737554	31.509581
580.106027	29623.256181	31.514599
580.727960	29677.345159	31.519616
581.387249	29720.374672	31.524634
582.272499	29777.952178	31.529652
582.662680	29828.748572	31.534669
583.441928	29866.032342	31.539687
584.026477	29920.175358	31.544704
584.941922	29964.031510	31.549722
585.100627	30007.415707	31.554740
585.912870	30056.268621	31.559757
586.667017	30087.308138	31.564775
587.121418	30139.285141	31.569792
587.929689	30184.329910	31.574810
588.638812	30226.990349	31.579828
588.922864	30276.156543	31.584845
589.560525	30313.868916	31.589863
589.914665	30361.462386	31.594880
590.736038	30408.838183	31.599898
591.251823	30450.297548	31.604916
591.569104	30497.129762	31.609933
592.311909	30545.405765	31.614951
593.017861	30597.832741	31.619968
593.540060	30645.589403	31.624986
594.483652	30685.061635	31.630004
594.681787	30737.651869	31.635021
595.319789	30778.586697	31.640039
595.881780	30831.302119	31.645056
596.406207	30876.933005	31.650074
597.073023	30918.533420	31.655092
597.648231	30966.006766	31.660109
598.612926	31010.478861	31.665127
599.113077	31067.061536	31.670144
599.306640	31105.666005	31.675162
600.125448	31154.562138	31.680180
600.139457	31195.657253	31.685197
600.981871	31239.567864	31.690215
601.624891	31291.412895	31.695232
601.980447	31333.224684	31.700250
602.745488	31383.603716	31.705268
603.107939	31433.438625	31.710285
603.944670	31476.143474	31.715303
604.420253	31530.594445	31.720320
604.736268	31579.400102	31.725338
605.512172	31626.885962	31.730356
605.893065	31686.950942	31.735373
606.950174	31731.829536	31.740391
607.432326	31788.655559	31.745408
607.966287	31842.075349	31.750426
608.386383	31890.761332	31.755444
608.968329	31951.496655	31.760461
609.524994	32003.764333	31.765479
610.189496	32052.673525	31.770496
610.951196	32116.810587	31.775514
611.782247	32169.433877	31.780532
612.528666	32218.577980	31.785549
612.943492	32270.350522	31.790567
613.502965	32323.315444	31.795584
614.093990	32386.336411	31.800602
614.987936	32432.332054	31.805620
615.486642	32478.898295	31.810637
616.256805	32536.418709	31.815655
616.816764	32598.520194	31.820672
617.234057	32647.807824	31.825690
618.339140	32690.317058	31.830708
618.393252	32753.141188	31.835725
618.993258	32801.361446	31.840743
620.044459	32862.748911	31.845760
620.774066	32907.897230	31.850778
621.332342	32965.192792	31.855796
621.520944	33024.918110	31.860813
622.396548	33077.857189	31.865831
623.108364	33135.209285	31.870848
623.604476	33184.528527	31.875866
624.507830	33234.840764	31.880884
625.262732	33287.255914	31.885901
626.054033	33332.542167	31.890919
626.407798	33379.643166	31.895936
626.943301	33427.163033	31.900954
628.091416	33472.318775	31.905972
628.431760	33529.914233	31.910989
629.152576	33579.840437	31.916007
629.417406	33625.045797	31.921024
629.637769	33689.609334	31.926042
630.404885	33734.648326	31.931060
631.117907	33797.631604	31.936077
632.005622	33861.875181	31.941095
632.888462	33905.196916	31.946112
633.483630	33943.619551	31.951130
634.158089	33983.799897	31.956148
634.390330	34039.000934	31.961165
635.333362	34077.335393	31.966183
636.012307	34120.582961	31.971200
636.180239	34164.878313	31.976218
636.776072	34204.780084	31.981236
637.528126	34261.626811	31.986253
637.973685	34308.830908	31.991271
638.433207	34365.664661	31.996288
639.126181	34417.232536	32.001306
639.854889	34467.611005	32.006324
640.309532	34519.533997	32.011341
640.835106	34573.574013	32.016359
641.722684	34628.283299	32.021376
642.170380	34677.198512	32.026394
642.962229	34739.059858	32.031412
643.513888	34805.309049	32.036429
644.173405	34857.131115	32.041447
644.990973	34909.596591	32.046464
645.816329	34960.120386	32.051482
646.671141	35015.275990	32.056500
646.876390	35078.168397	32.061517
647.717857	35121.539306	32.066535
648.662902	35175.448282	32.071552
648.983837	35236.686495	32.076570
649.850946	35280.632302	32.081588
650.121700	35334.174619	32.086605
650.814489	35393.514453	32.091623
651.663710	35459.657388	32.096640
652.120448	35517.096153	32.101658
653.146888	35569.639233	32.106676
653.475935	35634.615504	32.111693
654.003798	35693.895953	32.116711
654.922965	35745.219099	32.121728
655.266146	35799.870706	32.126746
656.466663	35859.618513	32.131764
656.936000	35915.235746	32.136781
657.625679	35967.032808	32.141799
658.273403	36025.757751	32.146816
658.676504	36090.616796	32.151834
659.770015	36132.748876	32.156852
659.992107	36198.485342	32.161869
660.714752	36258.239704	32.166887
661.576954	36319.599088	32.171904
662.167382	36381.426061	32.176922
662.715392	36438.564942	32.181940
663.316777	36494.883576	32.186957
664.040625	36549.150670	32.191975
664.875905	36623.011556	32.196992
665.016697	36678.942187	32.202010
665.801001	36735.221471	32.207028
666.816820	36807.726920	32.212045
667.216570	36861.698186	32.217063
668.048107	36927.717298	32.222080
668.688588	36983.955669	32.227098
669.618600	37035.025628	32.232116
670.179727	37080.962570	32.237133
670.477843	37133.765251	32.242151
671.035015	37196.784583	32.247168
671.753066	37250.053688	32.252186
672.385087	37292.046151	32.257204
673.058642	37357.322685	32.262221
673.652875	37414.705063	32.267239
674.581882	37471.050493	32.272256
674.991154	37535.267688	32.277274
675.795046	37585.367659	32.282292
676.559949	37655.138572	32.287309
676.928780	37711.668584	32.292327
677.948500	37774.711047	32.297344
678.563365	37836.586779	32.302362
679.453705	37898.612822	32.307380
679.631158	37963.075097	32.312397
680.310210	38029.939549	32.317415
681.482155	38085.314934	32.322432
682.041993	38148.069350	32.327450
682.819552	38206.114274	32.332468
683.100449	38266.581519	32.337485
683.854987	38336.115652	32.342503
685.070261	38389.941489	32.347520
685.414291	38465.615213	32.352538
686.269610	38514.267008	32.357556
687.201748	38577.100931	32.362573
687.586014	38642.322839	32.367591
688.512635	38698.748435	32.372608
689.187495	38764.651459	32.377626
689.770177	38817.485057	32.382644
690.503250	38890.042892	32.387661
691.225566	38937.026730	32.392679
691.865810	38988.885110	32.397696
692.345115	39069.032363	32.402714
693.324405	39129.475084	32.407732
694.198693	39201.206008	32.412749
694.309910	39260.128538	32.417767
695.028603	39323.721403	32.422784
695.791826	39390.065347	32.427802
696.625268	39438.716973	32.432820
697.152883	39512.216870	32.437837
698.030979	39569.597636	32.442855
698.893465	39635.857357	32.447872
699.711845	39702.433427	32.452890
700.741693	39754.115437	32.457908
701.325945	39816.974638	32.462925
701.783342	39881.101597	32.467943
702.722158	39935.228661	32.472960
703.055665	39996.133644	32.477978
703.898907	40053.417516	32.482996
704.266686	40117.835591	32.488013
705.115247	40178.159353	32.493031
706.271103	40234.864225	32.498048
706.350564	40295.110552	32.503066
707.297143	40343.689990	32.508084
708.265929	40401.749831	32.513101
709.064058	40463.378887	32.518119
709.742445	40510.563303	32.523136
709.991493	40565.183789	32.528154
710.735799	40614.751840	32.533172
711.070633	40676.146322	32.538189
711.791621	40731.487016	32.543207
712.732724	40790.889872	32.548224
713.088393	40860.147725	32.553242
713.802019	40908.182363	32.558260
714.584789	40985.746618	32.563277
715.174711	41049.975146	32.568295
715.928040	41117.953291	32.573312
716.419704	41191.849356	32.578330
717.046259	41254.795429	32.583348
717.638895	41330.946949	32.588365
718.463685	41411.414504	32.593383
719.517113	41476.889266	32.598400
719.902367	41554.333275	32.603418
721.219641	41620.482575	32.608436
721.866748	41676.970418	32.613453
722.716155	41753.448824	32.618471
723.338135	41820.914455	32.623488
724.127099	41889.189631	32.628506
725.189276	41943.946879	32.633524
725.630109	42012.369428	32.638541
726.051067	42078.871339	32.643559
727.133115	42140.511708	32.648576
727.801995	42219.503299	32.653594
728.558100	42284.627879	32.658612
729.678509	42358.409960	32.663629
729.967620	42428.791878	32.668647
730.650134	42485.920218	32.673664
731.348581	42571.895474	32.678682
732.110571	42630.601414	32.683700
732.621246	42700.441329	32.688717
733.550730	42771.533382	32.693735
734.982217	42842.290325	32.698752
735.128234	42913.867262	32.703770
736.161249	42987.079234	32.708788
736.632352	43045.435433	32.713805
737.357102	43123.649446	32.718823
738.665844	43184.525650	32.723840
739.157304	43246.557340	32.728858
740.015887	43305.622426	32.733876
740.627306	43364.581948	32.738893
741.655456	43435.377132	32.743911
742.846472	43492.317463	32.748928
743.064646	43559.327370	32.753946
743.717412	43620.975117	32.758964
744.416702	43674.984923	32.763981
745.677315	43744.816951	32.768999
746.217046	43801.530736	32.774016
746.927735	43856.775872	32.779034
747.893815	43912.018390	32.784052
748.327491	43961.841115	32.789069
748.539803	44018.033590	32.794087
749.316394	44069.568606	32.799104
750.156824	44127.904372	32.804122
750.546180	44189.435181	32.809140
751.013364	44259.979168	32.814157
751.730947	44336.862244	32.819175
752.313158	44399.498768	32.824192
753.038722	44486.485547	32.829210
753.972208	44551.751323	32.834228
754.787225	44626.456072	32.839245
755.438284	44700.647784	32.844263
756.372495	44758.680511	32.849280
757.024166	44839.352480	32.854298
757.801506	44910.786693	32.859316
758.764329	44992.047103	32.864333
759.235939	45070.726608	32.869351
760.352368	45133.712954	32.874368
761.294775	45205.267223	32.879386
761.852481	45271.829029	32.884404
762.852373	45341.343019	32.889421
763.384614	45423.080938	32.894439
764.541468	45485.267106	32.899456
765.100557	45564.546952	32.904474
765.747790	45637.225774	32.909492
766.877621	45700.950276	32.914509
767.380899	45777.299626	32.919527
768.110479	45839.854774	32.924544
768.828301	45920.230959	32.929562
769.204414	45989.597567	32.934580
769.922722	46072.946315	32.939597
770.979342	46158.910711	32.944615
771.858128	46228.381251	32.949632
772.653489	46315.798267	32.954650
773.387270	46391.757098	32.959668
774.399027	46463.160351	32.964685
775.096352	46543.836074	32.969703
775.924156	46601.850851	32.974720
776.878835	46688.275772	32.979738
777.566695	46751.266746	32.984756
778.154109	46824.704609	32.989773
778.760677	46918.430118	32.994791
779.870840	46983.168894	32.999808
780.458903	47064.268248	33.004826
780.900237	47149.511932	33.009844
782.037032	47210.909178	33.014861
783.023180	47283.010819	33.019879
783.651243	47363.313240	33.024896
784.631976	47438.707226	33.029914
785.518754	47515.328084	33.034932
786.444877	47584.733353	33.039949
787.010905	47660.440392	33.044967
788.278355	47726.125528	33.049984
788.938564	47797.211521	33.055002
789.463623	47862.280137	33.060020
790.466059	47912.875518	33.065037
791.175290	47975.656069	33.070055
791.460078	48035.579434	33.075072
792.466251	48110.123470	33.080090
793.273065	48171.150614	33.085108
793.993749	48224.000448	33.090125
794.589865	48303.485536	33.095143
795.417043	48366.964970	33.100160
796.240263	48438.917412	33.105178
796.675087	48508.227798	33.110196
797.973090	48573.387437	33.115213
798.816299	48658.842657	33.120231
799.748023	48731.627826	33.125248
800.214711	48801.994510	33.130266
800.974119	48876.984944	33.135284
801.667080	48946.019304	33.140301
802.166944	49038.252110	33.145319
803.010701	49098.882140	33.150336
804.037401	49168.978143	33.155354
804.525299	49254.082559	33.160372
805.766983	49344.905149	33.165389
806.373101	49431.518875	33.170407
807.222254	49503.127555	33.175424
807.847422	49589.246752	33.180442
808.878733	49665.980143	33.185460
810.114230	49737.269528	33.190477
810.608178	49836.673770	33.195495
811.412961	49896.646891	33.200512
812.392363	49971.935122	33.205530
812.937755	50049.508000	33.210548
813.939506	50134.105683	33.215565
814.633151	50215.780146	33.220583
815.470503	50302.276105	33.225600
816.278121	50393.760080	33.230618
817.005918	50468.099550	33.235636
818.490050	50547.491226	33.240653
818.649782	50633.626414	33.245671
819.316777	50722.429968	33.250688
820.588977	50801.771294	33.255706
821.197007	50892.387027	33.260724
822.110596	50970.100969	33.265741
822.682293	51051.662956	33.270759
823.452349	51132.931815	33.275776
824.457501	51219.291896	33.280794
825.354228	51303.479473	33.285812
826.339804	51387.463954	33.290829
826.946548	51477.609466	33.295847
827.787620	51571.549425	33.300864
828.877449	51635.711953	33.305882
829.452760	51734.043921	33.310900
830.366226	51814.507216	33.315917
830.984956	51904.403640	33.320935
831.678317	51987.279181	33.325952
832.807126	52073.207103	33.330970
833.091335	52160.065148	33.335988
834.497645	52234.351313	33.341005
835.009981	52318.390200	33.346023
835.760675	52390.890861	33.351040
836.827910	52465.348709	33.356058
837.428741	52552.205601	33.361076
838.239820	52624.492448	33.366093
839.029173	52713.059129	33.371111
839.916649	52797.864302	33.376128
840.776866	52882.667899	33.381146
841.484680	52971.479220	33.386164
842.383130	53052.635321	33.391181
843.138458	53142.232120	33.396199
844.067267	53228.588740	33.401216
845.044470	53322.408850	33.406234
845.757689	53413.553930	33.411252
847.239505	53489.584967	33.416269
847.985186	53568.564627	33.421287
848.809348	53650.120292	33.426304
849.786627	53734.634660	33.431322
850.344920	53814.513188	33.436340
851.520906	53895.824600	33.441357
852.472568	53972.936266	33.446375
853.197593	54062.911730	33.451392
854.278083	54148.352195	33.456410
854.662064	54230.899012	33.461428
855.610793	54313.110146	33.466445
856.416270	54400.855535	33.471463
856.916183	54482.898961	33.476480
858.220391	54574.157843	33.481498
858.922357	54669.524863	33.486516
859.858448	54751.815744	33.491533
860.896885	54845.561383	33.496551
861.485544	54939.331722	33.501568
862.556310	55024.818884	33.506586
863.607315	55115.590472	33.511604
864.195446	55200.315612	33.516621
865.269566	55288.158260	33.521639
866.068324	55367.064681	33.526656
867.216994	55465.325653	33.531674
867.839142	55558.361510	33.536692
868.704257	55631.115750	33.541709
869.814226	55730.694305	33.546727
870.206338	55807.789126	33.551744
870.980241	55901.585430	33.556762
871.771938	55996.799892	33.561780
872.705986	56085.423103	33.566797
873.667573	56188.459088	33.571815
874.443688	56282.638952	33.576832
875.770298	56368.612551	33.581850
876.214479	56464.298263	33.586868
877.443963	56553.751156	33.591885
878.462823	56632.362836	33.596903
879.281250	56718.611493	33.601920
880.169129	56805.727103	33.606938
880.880092	56888.896812	33.611956
881.463424	56967.456102	33.616973
882.366664	57059.697197	33.621991
883.208372	57141.552930	33.627008
884.454663	57219.834190	33.632026
884.824026	57308.651004	33.637044
885.930548	57384.688541	33.642061
886.782787	57477.766956	33.647079
887.396326	57568.585555	33.652096
888.203371	57654.284778	33.657114
888.922141	57751.606676	33.662132
889.803851	57853.730219	33.667149
890.536258	57943.976116	33.672167
891.470466	58043.067928	33.677184
892.143128	58136.257154	33.682202
893.151211	58241.873374	33.687220
894.162344	58341.649100	33.692237
895.113792	58438.719751	33.697255
896.198463	58545.541001	33.702272
897.281385	58627.882706	33.707290
898.476390	58730.419021	33.712308
899.815319	58823.417299	33.717325
900.620616	58911.275804	33.722343
901.450057	59000.810512	33.727360
902.728363	59085.772055	33.732378
903.202391	59179.582204	33.737396
904.104596	59274.874911	33.742413
904.872507	59360.199903	33.747431
906.128022	59453.836587	33.752448
907.081431	59538.826630	33.757466
907.472855	59637.520765	33.762484
908.523753	59729.669567	33.767501
909.315857	59833.289560	33.772519
910.227855	59927.387413	33.777536
911.237618	60015.884800	33.782554
912.060080	60111.169208	33.787572
912.925596	60217.116115	33.792589
914.402674	60306.490912	33.797607
914.604835	60406.946324	33.802624
915.532733	60496.759875	33.807642
916.921450	60599.133569	33.812660
917.915664	60696.468089	33.817677
918.996334	60787.452259	33.822695
919.707864	60887.393474	33.827712
921.166120	60971.476133	33.832730
921.487363	61073.542295	33.837748
922.537848	61168.353747	33.842765
923.740691	61254.458099	33.847783
924.486407	61342.135425	33.852800
925.388136	61438.395979	33.857818
925.859492	61529.613298	33.862836
926.903354	61630.816010	33.867853
927.811314	61733.704972	33.872871
928.323874	61824.828749	33.877888
929.547091	61920.260678	33.882906
930.468512	62004.019703	33.887924
931.307686	62100.719883	33.892941
932.817223	62181.976801	33.897959
933.356526	62272.106955	33.902976
934.428585	62364.006395	33.907994
935.162124	62448.640405	33.913012
936.081977	62534.839840	33.918029
936.774796	62625.032516	33.923047
937.353208	62728.134053	33.928064
938.830652	62817.400741	33.933082
939.550206	62926.351328	33.938100
940.088125	63026.031495	33.943117
941.167874	63123.033364	33.948135
941.789410	63228.710759	33.953152
942.798319	63338.034523	33.958170
943.825909	63439.432666	33.963188
944.569659	63548.796665	33.968205
945.736463	63657.130812	33.973223
946.458620	63769.606966	33.978240
947.631654	63871.615878	33.983258
948.817480	63984.499562	33.988276
949.443463	64099.547811	33.993293
950.772207	64210.682647	33.998311
951.235612	64312.876282	34.003328
952.773062	64425.656116	34.008346
953.648623	64535.352200	34.013364
954.734094	64638.683452	34.018381
955.735039	64741.725524	34.023399
956.798510	64848.794354	34.028416
958.317352	64940.499385	34.033434
959.335203	65045.744824	34.038452
960.168789	65140.114806	34.043469
961.389699	65235.825900	34.048487
962.060229	65337.180391	34.053504
963.024244	65437.635999	34.058522
964.196888	65532.456145	34.063540
965.342816	65628.888586	34.068557
966.470337	65722.980967	34.073575
966.748537	65825.051054	34.078592
967.717853	65920.619244	34.083610
968.923259	66020.802630	34.088628
969.900843	66118.066531	34.093645
971.212317	66208.180890	34.098663
972.090863	66311.711994	34.103680
972.976583	66403.764774	34.108698
973.677376	66505.044804	34.113716
974.664690	66599.353281	34.118733
975.611262	66704.789704	34.123751
976.256275	66820.239728	34.128768
977.764449	66910.572449	34.133786
978.410162	67021.895391	34.138804
979.453643	67125.606771	34.143821
980.350723	67225.223227	34.148839
981.427069	67340.276097	34.153856
982.413108	67434.143491	34.158874
983.126994	67535.426835	34.163892
984.268311	67625.536977	34.168909
985.460789	67706.668853	34.173927
985.955272	67816.933843	34.178944
987.015541	67890.986852	34.183962
988.097803	67986.673647	34.188980
988.780500	68096.373309	34.193997
989.768335	68183.907684	34.199015
990.645577	68294.563040	34.204032
991.643960	68395.154916	34.209050
992.811741	68496.529013	34.214068
993.758354	68600.270002	34.219085
994.944750	68701.869640	34.224103
995.601110	68811.406943	34.229120
996.874638	68913.132812	34.234138
997.942814	69017.330511	34.239156
998.638565	69127.097074	34.244173
999.617072	69225.801074	34.249191
1000.670166	69331.279037	34.254208
1001.997005	69438.129228	34.259226
1003.100631	69537.459321	34.264244
1004.066183	69646.585689	34.269261
1005.338351	69747.418977	34.274279
1006.428839	69851.882928	34.279296
1007.346305	69948.704890	34.284314
1008.700479	70054.998116	34.289332
1009.143894	70158.827408	34.294349
1010.401912	70255.249224	34.299367
1011.256294	70368.049155	34.304384
1012.073939	70472.307078	34.309402
1013.159850	70575.771019	34.314420
1014.062058	70687.762763	34.319437
1015.353713	70777.136947	34.324455
1016.028862	70894.195325	34.329472
1016.480225	71003.316233	34.334490
1017.746305	71125.305085	34.339508
1018.730000	71245.406165	34.344525
1020.002623	71354.429988	34.349543
1021.124789	71470.378141	34.354560
1022.469489	71587.555288	34.359578
1023.383042	71689.258020	34.364596
1024.009350	71817.406085	34.369613
1025.354745	71924.317382	34.374631
1026.219960	72044.334739	34.379648
1027.250008	72156.680959	34.384666
1028.185939	72270.230710	34.389684
1028.898943	72389.332867	34.394701
1030.203598	72506.180602	34.399719
1031.524856	72617.655351	34.404736
1032.770752	72742.677794	34.409754
1033.673065	72859.060805	34.414772
1034.352794	72967.492712	34.419789
1035.666169	73071.837142	34.424807
1036.998146	73201.126742	34.429824
1038.008360	73301.672291	34.434842
1039.257638	73397.586334	34.439860
1039.944819	73504.042092	34.444877
1040.956497	73599.318744	34.449895
1041.951947	73695.110286	34.454912
1043.203400	73797.054424	34.459930
1043.939141	73892.964049	34.464948
1044.877845	73993.865696	34.469965
1046.082221	74102.953368	34.474983
1046.575613	74215.282791	34.480000
1047.740720	74322.134527	34.485018
1048.701717	74422.655624	34.490036
1049.426676	74543.601362	34.495053
1050.894693	74650.438272	34.500071
1051.798662	74773.170621	34.505088
1052.739821	74893.300457	34.510106
1053.795425	75014.215402	34.515124
1054.790226	75137.093516	34.520141
1055.746352	75249.405684	34.525159
1056.648304	75382.664358	34.530176
1057.382529	75507.557925	34.535194
1058.676841	75630.663166	34.540212
1059.667809	75767.442997	34.545229
1061.230427	75885.552361	34.550247
1062.148104	76025.315940	34.555264
1063.378137	76153.857096	34.560282
1064.494223	76272.842369	34.565300
1065.556520	76401.689852	34.570317
1067.133946	76516.627882	34.575335
1067.800612	76632.798458	34.580352
1068.946441	76758.051412	34.585370
1070.578145	76874.208949	34.590388
1071.311787	76997.651830	34.595405
1072.526205	77120.342736	34.600423
1073.514285	77236.964953	34.605440
1074.527749	77359.000340	34.610458
1075.847284	77478.763011	34.615476
1076.682457	77606.567142	34.620493
1077.924882	77720.882651	34.625511
1079.139484	77844.633407	34.630528
1080.138138	77974.354237	34.635546
1081.313095	78090.250037	34.640564
1082.285386	78214.844280	34.645581
1083.404356	78321.699180	34.650599
1084.643832	78449.855134	34.655616
1085.806357	78563.031374	34.660634
1087.207482	78687.863698	34.665652
1087.638835	78807.977657	34.670669
1088.702480	78921.506602	34.675687
1089.752678	79046.156716	34.680704
1091.026903	79173.660617	34.685722
1092.577896	79290.223990	34.690740
1093.527878	79403.659896	34.695757
1094.676454	79526.363058	34.700775
1095.611675	79641.800063	34.705792
1096.597041	79754.796122	34.710810
1097.594268	79859.099377	34.715828
1098.499384	79973.228231	34.720845
1099.719106	80072.237986	34.725863
1100.954685	80193.578550	34.730880
1101.657795	80302.406235	34.735898
1103.091722	80417.363716	34.740916
1103.958868	80529.150158	34.745933
1105.055785	80634.503456	34.750951
1106.027537	80760.213101	34.755968
1106.697729	80882.507314	34.760986
1108.150837	80987.647735	34.766004
1108.975117	81122.422714	34.771021
1109.905898	81251.555459	34.776039
1111.115811	81378.577465	34.781056
1112.363572	81513.154887	34.786074
1113.227353	81637.559465	34.791092
1114.146053	81770.838039	34.796109
1115.612314	81888.934092	34.801127
1116.682185	82033.575754	34.806144
1117.767270	82170.010276	34.811162
1119.063992	82298.484425	34.816180
1119.893411	82440.423449	34.821197
1121.001078	82568.025283	34.826215
1122.176356	82705.055860	34.831232
1123.007167	82848.628498	34.836250
1124.678830	82983.824449	34.841268
1125.680715	83130.867920	34.846285
1126.785504	83265.384521	34.851303
1127.934253	83403.144599	34.856320
1129.277709	83536.992771	34.861338
1130.938176	83667.035963	34.866356
1131.753921	83796.449268	34.871373
1133.322879	83929.227223	34.876391
1134.217233	84048.336795	34.881408
1135.423068	84188.090804	34.886426
1136.721677	84316.469517	34.891444
1137.517845	84453.976398	34.896461
1138.959659	84576.169478	34.901479
1140.258431	84716.101878	34.906496
1141.410129	84842.174107	34.911514
1142.607239	84971.154612	34.916532
1143.576487	85117.199160	34.921549
1144.569921	85240.826746	34.926567
1145.985949	85369.458729	34.931584
1147.111712	85502.152629	34.936602
1148.549478	85610.872077	34.941620
1149.639727	85740.544466	34.946637
1150.755469	85858.187391	34.951655
1152.015855	85991.571106	34.956672
1152.947555	86121.068684	34.961690
1154.150326	86244.738371	34.966708
1155.218926	86371.439889	34.971725
1156.576978	86497.236196	34.976743
1157.904708	86615.836000	34.981760
1159.108196	86739.729749	34.986778
1160.109950	86841.676789	34.991796
1160.758498	86962.631236	34.996813
1161.855698	87072.670606	35.001831
1163.158287	87188.033735	35.006848
1164.106530	87312.382390	35.011866
1165.337314	87425.304750	35.016884
1166.312137	87552.679472	35.021901
1166.925237	87695.870521	35.026919
1168.399231	87816.818690	35.031936
1169.075395	87951.022041	35.036954
1170.347477	88089.235489	35.041972
1171.556694	88231.222372	35.046989
1172.830723	88362.816434	35.052007
1174.333133	88510.677489	35.057024
1175.031754	88650.478093	35.062042
1176.474581	88780.466927	35.067060
1177.072147	88925.641615	35.072077
1178.358150	89067.621781	35.077095
1179.709809	89215.246012	35.082112
1180.603295	89357.846983	35.087130
1182.055156	89501.454171	35.092148
1183.269163	89656.767965	35.097165
1184.440425	89805.765583	35.102183
1185.727040	89948.175120	35.107200
1186.569265	90106.068221	35.112218
1187.994142	90248.008721	35.117236
1189.207581	90399.330998	35.122253
1190.378989	90562.417871	35.127271
1192.080924	90701.382799	35.132288
1193.416707	90846.712226	35.137306
1194.719450	90982.763620	35.142324
1196.292776	91123.762843	35.147341
1197.551398	91258.077410	35.152359
1199.041496	91391.672952	35.157376
1200.386682	91530.908567	35.162394
1201.118578	91660.730338	35.167412
1202.458513	91792.499077	35.172429
1203.773360	91932.621185	35.177447
1204.981597	92064.861544	35.182464
1206.194643	92194.780742	35.187482
1207.592867	92322.419638	35.192500
1208.615238	92466.095572	35.197517
1209.757443	92602.606271	35.202535
1210.638352	92738.640706	35.207552
1211.773590	92886.975550	35.212570
1213.005880	93010.723321	35.217588
1214.570378	93158.036668	35.222605
1215.485456	93294.922966	35.227623
1217.105861	93436.119247	35.232640
1218.102896	93580.584424	35.237658
1219.136095	93708.611918	35.242676
1220.364332	93852.839705	35.247693
1221.361989	94003.208974	35.252711
1223.240420	94130.218996	35.257728
1223.841343	94284.916494	35.262746
1225.180310	94408.642437	35.267764
1226.304543	94533.042069	35.272781
1227.352920	94669.105965	35.277799
1228.730256	94791.037820	35.282816
1230.013425	94930.114874	35.287834
1231.049707	95057.959850	35.292852
1232.249465	95200.372770	35.297869
1233.376229	95329.697759	35.302887
1234.787470	95460.357274	35.307904
1235.598999	95604.694223	35.312922
1236.962852	95737.918482	35.317940
1237.980782	95887.474825	35.322957
1239.430184	96028.436327	35.327975
1240.738937	96174.696862	35.332992
1242.168915	96321.014988	35.338010
1243.235424	96457.036217	35.343028
1244.339925	96610.973820	35.348045
1245.990360	96753.647551	35.353063
1247.072276	96897.924486	35.358080
1248.248358	97059.135094	35.363098
1249.427935	97194.655670	35.368116
1251.032939	97343.173073	35.373133
1251.938852	97494.997329	35.378151
1253.576978	97632.971814	35.383168
1254.573587	97790.926466	35.388186
1255.776898	97926.460286	35.393204
1257.216925	98088.756011	35.398221
1258.308774	98237.316529	35.403239
1260.176055	98384.552728	35.408256
1261.195287	98541.104492	35.413274
1262.269204	98675.442300	35.418292
1263.947027	98834.523254	35.423309
1265.157756	98980.614973	35.428327
1266.560867	99130.960230	35.433344
1267.714324	99282.820286	35.438362
1268.857354	99428.843370	35.443380
1270.071798	99579.898520	35.448397
1270.954604	99731.076967	35.453415
1272.642584	99880.521394	35.458432
1273.529287	100041.292868	35.463450
1275.051478	100199.452635	35.468468
1276.260095	100350.153118	35.473485
1277.918776	100504.503381	35.478503
1279.421619	100652.463732	35.483520
1280.382087	100814.158943	35.488538
1281.925943	100958.805621	35.493556
1283.372168	101106.619692	35.498573
1284.146642	101254.408595	35.503591
1285.946619	101408.312166	35.508608
1287.642509	101546.705921	35.513626
1288.988371	101693.229909	35.518644
1290.115300	101830.545207	35.523661
1291.424226	101979.240852	35.528679
1293.004827	102109.266024	35.533696
1294.468088	102241.987128	35.538714
1295.321604	102364.188187	35.543732
1296.671181	102497.789365	35.548749
1297.746832	102623.797348	35.553767
1299.137200	102746.997115	35.558784
1300.079269	102872.458173	35.563802
1301.311844	103005.808752	35.568820
1302.668237	103133.514994	35.573837
1303.419778	103272.929641	35.578855
1304.980480	103411.678647	35.583872
1305.948044	103566.038788	35.588890
1307.385498	103705.916502	35.593908
1308.507798	103850.508865	35.598925
1309.295142	104006.286358	35.603943
1311.057627	104148.861413	35.608960
1312.221909	104304.783468	35.613978
1313.456814	104462.024240	35.618996
1314.726731	104625.031811	35.624013
1315.894418	104788.227612	35.629031
1317.547780	104943.411679	35.634048
1318.735769	105110.548991	35.639066
1319.735931	105265.206133	35.644084
1320.979200	105430.318156	35.649101
1322.039331	105591.315287	35.654119
1324.154327	105763.923211	35.659136
1325.472408	105933.355526	35.664154
1326.693425	106102.563980	35.669172
1328.010628	106262.847626	35.674189
1329.345201	106435.831244	35.679207
1330.743758	106592.357587	35.684224
1331.734876	106774.492604	35.689242
1333.164669	106945.015527	35.694260
1335.157852	107111.830023	35.699277
1336.482585	107279.416438	35.704295
1338.028170	107435.526188	35.709312
1339.127607	107598.486192	35.714330
1340.578522	107767.473641	35.719348
1342.125235	107928.763552	35.724365
1343.498298	108088.240362	35.729383
1344.715058	108259.230483	35.734400
1346.448407	108419.487672	35.739418
1347.862099	108586.815848	35.744436
1349.693033	108737.337914	35.749453
1350.454168	108897.354006	35.754471
1351.938418	109046.376063	35.759488
1353.294912	109203.267795	35.764506
1354.380940	109377.476578	35.769524
1356.206533	109530.048811	35.774541
1357.458909	109689.992044	35.779559
1358.899051	109836.633378	35.784576
1359.989194	110000.971827	35.789594
1361.522843	110159.525228	35.794612
1363.204457	110309.378137	35.799629
1364.247524	110469.568601	35.804647
1365.371486	110624.841682	35.809664
1367.165490	110777.230487	35.814682
1368.262432	110918.381581	35.819700
1369.517798	111065.319144	35.824717
1370.772207	111200.104288	35.829735
1372.112425	111343.592881	35.834752
1373.147407	111502.531687	35.839770
1374.328620	111649.826333	35.844788
1375.838423	111800.823377	35.849805
1376.885903	111959.452957	35.854823
1378.251920	112122.160199	35.859840
1379.575130	112276.063678	35.864858
1381.239064	112452.462273	35.869876
1382.557992	112600.519303	35.874893
1383.846530	112772.352383	35.879911
1385.250562	112930.216179	35.884928
1386.615767	113095.538027	35.889946
1387.742823	113271.217434	35.894964
1389.639097	113430.158321	35.899981
1390.694503	113615.359923	35.904999
1392.364333	113780.580923	35.910016
1393.873261	113948.728002	35.915034
1395.123180	114114.853565	35.920052
1396.571261	114280.492932	35.925069
1397.732629	114459.448183	35.930087
1399.285689	114622.762401	35.935104
1400.680259	114805.145995	35.940122
1402.110837	114983.163212	35.945140
1403.897809	115146.405670	35.950157
1405.046642	115330.839004	35.955175
1406.688259	115503.185464	35.960192
1408.527750	115673.665653	35.965210
1409.742226	115849.133895	35.970228
1410.981384	116011.380019	35.975245
1412.324693	116187.406260	35.980263
1414.040620	116361.278882	35.985280
1415.446362	116538.766475	35.990298
1416.861210	116713.012227	35.995316
1418.277043	116883.314580	36.000333
1419.621475	117058.384287	36.005351
1421.062826	117224.759396	36.010368
1422.752924	117392.115432	36.015386
1423.920495	117575.074129	36.020404
1425.388587	117743.132536	36.025421
1426.535950	117927.635521	36.030439
1427.989449	118099.890101	36.035456
1429.533727	118280.197985	36.040474
1430.780269	118473.692789	36.045492
1432.799221	118631.133458	36.050509
1434.050954	118816.816592	36.055527
1435.470180	118981.047411	36.060544
1437.183377	119158.314284	36.065562
1438.665787	119333.421848	36.070580
1439.897472	119498.774834	36.075597
1441.518786	119675.344319	36.080615
1442.904131	119836.527559	36.085632
1444.385423	120011.576544	36.090650
1445.858840	120177.522315	36.095668
1447.218399	120318.373755	36.100685
1448.298573	120483.573423	36.105703
1449.862074	120638.249107	36.110720
1451.295999	120800.937659	36.115738
1452.391013	120959.818330	36.120756
1453.678068	121129.472500	36.125773
1455.377833	121296.503901	36.130791
1456.431392	121464.348257	36.135808
1457.915552	121629.111003	36.140826
1459.247037	121819.520517	36.145844
1460.790673	121985.301913	36.150861
1462.105173	122172.993659	36.155879
1463.684174	122356.503145	36.160896
1464.948291	122534.453133	36.165914
1466.261351	122728.735073	36.170932
1467.959294	122901.894364	36.175949
1469.575323	123099.436610	36.180967
1471.132931	123268.415564	36.185984
1472.697733	123456.887229	36.191002
1474.067029	123650.369007	36.196020
1475.646485	123830.329448	36.201037
1477.139596	124011.014120	36.206055
1478.765857	124204.395753	36.211072
1480.290778	124392.715683	36.216090
1481.625260	124580.826523	36.221108
1483.243426	124763.637019	36.226125
1484.438682	124955.762541	36.231143
1486.349295	125139.871793	36.236160
1487.690491	125333.408155	36.241178
1488.902794	125535.098497	36.246196
1490.518713	125713.406381	36.251213
1492.146343	125906.850674	36.256231
1493.815203	126108.510760	36.261248
1495.471361	126285.447962	36.266266
1496.886474	126480.564168	36.271284
1498.502891	126664.477161	36.276301
1500.022751	126870.144115	36.281319
1501.751813	127055.131250	36.286336
1503.698056	127230.913765	36.291354
1504.562838	127426.364827	36.296372
1506.741710	127600.567300	36.301389
1507.917302	127786.280678	36.306407
1509.664187	127975.426267	36.311424
1511.339944	128158.947161	36.316442
1512.947381	128340.643247	36.321460
1514.542854	128516.325019	36.326477
1515.797426	128695.925893	36.331495
1517.199571	128879.444364	36.336512
1518.898667	129055.037088	36.341530
1519.918397	129242.153209	36.346548
1521.840504	129418.371577	36.351565
1523.448836	129599.543699	36.356583
1524.784958	129789.007634	36.361600
1526.348956	129956.202751	36.366618
1528.052188	130126.962073	36.371636
1529.443764	130293.236423	36.376653
1530.649160	130460.174788	36.381671
1532.149393	130629.867212	36.386688
1534.021013	130792.977001	36.391706
1534.664427	130959.652860	36.396724
1536.511021	131133.461531	36.401741
1537.794659	131305.333570	36.406759
1539.235390	131492.777959	36.411776
1540.774874	131668.260416	36.416794
1542.279371	131866.403025	36.421812
1543.768606	132040.578121	36.426829
1545.111534	132233.098216	36.431847
1546.322186	132427.655155	36.436864
1548.252896	132603.866815	36.441882
1549.593523	132808.009637	36.446900
1551.283488	132999.985672	36.451917
1552.873172	133199.467099	36.456935
1554.320645	133394.335129	36.461952
1556.183784	133593.750539	36.466970
1557.793707	133798.009714	36.471988
1559.334949	134000.950828	36.477005
1560.708100	134192.592392	36.482023
1562.357959	134386.662105	36.487040
1564.146907	134587.059184	36.492058
1565.124345	134804.134925	36.497076
1566.908493	134998.225440	36.502093
1568.906064	135203.231299	36.507111
1570.473994	135402.541396	36.512128
1572.251991	135611.031610	36.517146
1573.619360	135825.303377	36.522164
1575.430337	136017.381685	36.527181
1576.975381	136210.567914	36.532199
1578.665070	136415.327100	36.537216
1580.600452	136623.064601	36.542234
1582.301759	136809.057710	36.547252
1583.684751	137014.097889	36.552269
1585.458401	137199.080894	36.557287
1586.862097	137405.679185	36.562304
1588.707970	137609.065982	36.567322
1590.268782	137806.530775	36.572340
1591.822648	137989.120557	36.577357
1593.342382	138188.102443	36.582375
1594.966188	138390.072546	36.587392
1597.110758	138570.291039	36.592410
1598.427011	138779.333297	36.597428
1599.953172	138971.805619	36.602445
1601.804119	139160.983338	36.607463
1603.435940	139349.740828	36.612480
1605.097339	139547.682805	36.617498
1606.813231	139734.427026	36.622516
1608.124199	139919.386421	36.627533
1610.038144	140111.931241	36.632551
1611.726979	140298.835357	36.637568
1613.649230	140473.917228	36.642586
1614.941736	140644.778437	36.647604
1616.568634	140805.283859	36.652621
1618.462762	140969.118902	36.657639
1619.674876	141139.653490	36.662656
1621.398196	141301.806504	36.667674
1622.678427	141477.743905	36.672692
1624.443289	141639.055649	36.677709
1625.496704	141817.489786	36.682727
1626.894102	142007.669953	36.687744
1628.565316	142177.579809	36.692762
1630.360636	142369.181926	36.697780
1631.612291	142560.022393	36.702797
1633.074999	142747.522511	36.707815
1634.917250	142945.052419	36.712832
1636.533645	143147.930117	36.717850
1637.638091	143348.482256	36.722868
1639.576606	143551.032622	36.727885
1641.269273	143750.746168	36.732903
1642.424883	143959.469431	36.737920
1644.320959	144166.251324	36.742938
1646.002899	144381.079263	36.747956
1647.758827	144593.666108	36.752973
1649.482491	144806.158129	36.757991
1650.761522	145011.053609	36.763008
1652.512948	145218.157007	36.768026
1654.484490	145439.283988	36.773044
1656.334439	145646.121069	36.778061
1658.309417	145855.310020	36.783079
1659.867637	146066.138336	36.788096
1661.944500	146269.977370	36.793114
1663.821726	146476.612779	36.798132
1665.104606	146671.567882	36.803149
1667.283959	146867.953687	36.808167
1668.949890	147079.595626	36.813184
1670.509730	147275.765421	36.818202
1671.875429	147483.743580	36.823220
1673.625479	147688.429585	36.828237
1675.511395	147887.758524	36.833255
1676.946638	148099.063583	36.838272
1678.844845	148310.258504	36.843290
1680.539073	148505.337017	36.848308
1682.524932	148714.150135	36.853325
1684.392822	148910.585318	36.858343
1685.980455	149105.912592	36.863360
1688.154325	149295.024952	36.868378
1689.518393	149489.642101	36.873396
1691.310790	149690.138034	36.878413
1693.107849	149881.126498	36.883431
1694.491063	150089.030022	36.888448
1696.084260	150281.092753	36.893466
1697.858165	150475.612725	36.898484
1699.496346	150692.696193	36.903501
1701.268453	150883.187405	36.908519
1702.847288	151090.318281	36.913536
1704.600982	151273.398201	36.918554
1706.241888	151467.869134	36.923572
1707.530723	151651.392625	36.928589
1709.305367	151827.043013	36.933607
1710.686358	152021.216178	36.938624
1712.503725	152207.321266	36.943642
1714.168603	152399.156834	36.948660
1715.654836	152594.749309	36.953677
1717.226654	152778.031288	36.958695
1718.959988	152987.926143	36.963712
1720.519147	153181.760870	36.968730
1722.210349	153396.584278	36.973748
1723.726371	153604.932692	36.978765
1725.707148	153809.468378	36.983783
1726.941916	154023.696302	36.988800
1728.810376	154231.472835	36.993818
1730.510400	154459.183495	36.998836
1732.377623	154670.779335	37.003853
1733.939772	154898.223233	37.008871
1735.701611	155121.795134	37.013888
1737.246450	155337.034570	37.018906
1739.017443	155566.681379	37.023924
1740.619815	155798.512033	37.028941
1743.100681	156016.345970	37.033959
1744.746015	156250.848286	37.038976
1746.609849	156474.121260	37.043994
1748.478748	156692.868170	37.049012
1750.370072	156921.769568	37.054029
1752.052899	157146.812814	37.059047
1753.747015	157375.279375	37.064064
1755.309266	157600.509567	37.069082
1757.382462	157825.393833	37.074100
1758.967085	158053.438450	37.079117
1761.012106	158281.360761	37.084135
1762.907328	158503.411893	37.089152
1764.724335	158739.679162	37.094170
1766.778454	158957.066852	37.099188
1768.163177	159184.478530	37.104205
1770.240786	159404.870624	37.109223
1772.163957	159630.132741	37.114240
1774.290453	159841.769962	37.119258
1775.696972	160066.102398	37.124276
1777.908508	160285.007742	37.129293
1779.843414	160494.536171	37.134311
1781.505301	160719.009753	37.139328
1783.257955	160933.946599	37.144346
1785.246351	161144.548299	37.149364
1786.760519	161358.777357	37.154381
1788.913666	161578.245252	37.159399
1790.657244	161796.536695	37.164416
1792.248504	162007.739153	37.169434
1794.146766	162226.541297	37.174452
1796.055468	162441.373665	37.179469
1798.064736	162643.027408	37.184487
1799.488866	162860.982873	37.189504
1801.447976	163074.733032	37.194522
1802.973938	163257.113918	37.199540
1804.454114	163458.577175	37.204557
1806.339157	163658.556861	37.209575
1807.900836	163852.146288	37.214592
1809.409726	164043.741282	37.219610
1811.303857	164246.221203	37.224628
1812.533581	164475.048113	37.229645
1814.600960	164670.451322	37.234663
1816.034059	164893.756939	37.239680
1817.867817	165110.823755	37.244698
1819.683809	165331.242967	37.249716
1821.215383	165562.007256	37.254733
1823.267784	165787.160483	37.259751
1825.011861	166030.298041	37.264768
1826.775835	166256.375026	37.269786
1829.071586	166485.768121	37.274804
1830.836027	166716.198204	37.279821
1832.885119	166939.151997	37.284839
1834.522616	167172.484186	37.289856
1836.108731	167411.622408	37.294874
1838.056061	167644.730777	37.299892
1839.874302	167882.084784	37.304909
1841.525594	168122.625063	37.309927
1843.805254	168369.358395	37.314944
1845.617510	168604.726484	37.319962
1847.494067	168834.060857	37.324980
1848.784811	169090.329373	37.329997
1850.962656	169324.362767	37.335015
1853.093882	169567.563107	37.340032
1854.832189	169810.155063	37.345050
1857.008739	170060.606832	37.350068
1858.665265	170298.546924	37.355085
1860.914435	170537.891220	37.360103
1862.674209	170782.312457	37.365120
1864.706739	171024.332561	37.370138
1866.562031	171268.310403	37.375156
1868.273106	171513.302082	37.380173
1870.557244	171754.627156	37.385191
1872.619935	171989.684328	37.390208
1874.180907	172235.363957	37.395226
1876.126199	172472.484960	37.400244
1878.034437	172707.989535	37.405261
1880.177459	172951.437410	37.410279
1882.005305	173210.007226	37.415296
1883.974868	173450.326976	37.420314
1886.186790	173682.782633	37.425332
1888.023316	173922.124158	37.430349
1890.004789	174153.870655	37.435367
1892.047917	174382.386478	37.440384
1893.922414	174625.874461	37.445402
1896.201236	174851.107922	37.450420
1897.761960	175085.197337	37.455437
1899.686446	175311.517160	37.460455
1901.389961	175547.540254	37.465472
1903.305691	175767.317874	37.470490
1905.533617	175965.480223	37.475508
1906.876671	176177.041313	37.480525
1909.202533	176381.102033	37.485543
1911.022759	176587.844753	37.490560
1912.695721	176800.764914	37.495578
1914.451364	177010.932717	37.500596
1916.321795	177223.176696	37.505613
1918.115917	177445.380373	37.510631
1919.730939	177665.406128	37.515648
1921.653640	177889.976919	37.520666
1923.876562	178108.652541	37.525684
1925.004120	178328.048655	37.530701
1927.175730	178558.647990	37.535719
1928.972298	178801.640131	37.540736
1930.651058	179037.864630	37.545754
1932.881948	179275.182773	37.550772
1934.303763	179531.420799	37.555789
1936.513391	179770.584773	37.560807
1938.125781	180009.273906	37.565824
1940.040981	180275.499418	37.570842
1941.976017	180516.068718	37.575860
1944.061873	180773.198473	37.580877
1946.397964	181020.025517	37.585895
1948.561529	181276.448107	37.590912
1950.442863	181525.824353	37.595930
1952.895826	181767.409626	37.600948
1954.621571	182026.862452	37.605965
1956.725419	182270.117307	37.610983
1958.774836	182516.287788	37.616000
1960.389712	182764.723692	37.621018
1962.936776	183008.952777	37.626036
1964.441694	183259.870489	37.631053
1966.517984	183514.036090	37.636071
1968.723759	183750.583337	37.641088
1970.759521	184002.195038	37.646106
1972.699645	184258.810057	37.651124
1974.592958	184517.971763	37.656141
1976.846947	184755.709446	37.661159
1978.580236	185006.118560	37.666176
1980.427922	185272.346979	37.671194
1982.824206	185516.106134	37.676212
1984.614806	185767.525508	37.681229
1986.807386	186025.176423	37.686247
1989.039893	186279.002939	37.691264
1990.837384	186521.986902	37.696282
1993.028565	186780.682834	37.701300
1994.631487	187039.219750	37.706317
1996.831537	187285.823880	37.711335
1998.795638	187535.360026	37.716352
2000.891982	187792.376235	37.721370
2002.932102	188033.844943	37.726388
2004.957575	188287.601127	37.731405
2006.759589	188537.777471	37.736423
2008.849291	188788.264832	37.741440
2011.023593	189043.778110	37.746458
2012.908529	189267.384618	37.751476
2014.909402	189497.686964	37.756493
2016.661818	189723.055215	37.761511
2018.696175	189947.516860	37.766528
2020.549113	190188.049119	37.771546
2022.726108	190410.548667	37.776564
2024.491179	190648.026060	37.781581
2026.640097	190880.811638	37.786599
2028.497349	191116.233516	37.791616
2030.004350	191368.362430	37.796634
2032.273678	191606.792499	37.801652
2033.637189	191873.528597	37.806669
2035.879627	192123.552282	37.811687
2037.864715	192382.070316	37.816704
2039.835150	192647.902125	37.821722
2042.331204	192901.557278	37.826740
2044.729831	193159.759970	37.831757
2046.384835	193420.721757	37.836775
2048.514487	193678.297167	37.841792
2050.488693	193940.543639	37.846810
2052.774456	194202.564382	37.851828
2054.981338	194463.418687	37.856845
2057.153479	194724.685985	37.861863
2059.374343	194978.788771	37.866880
2060.982122	195245.009200	37.871898
2063.658834	195497.595412	37.876916
2066.021042	195777.368084	37.881933
2067.600667	196033.468932	37.886951
2070.194975	196289.740107	37.891968
2072.204216	196556.081355	37.896986
2074.173320	196806.717423	37.902004
2076.304563	197073.816203	37.907021
2078.594760	197322.994993	37.912039
2080.900323	197576.970247	37.917056
2082.913312	197836.032028	37.922074
2085.328417	198085.397710	37.927092
2087.746526	198344.600817	37.932109
2089.342813	198596.434207	37.937127
2091.741439	198840.449780	37.942144
2094.189514	199092.416966	37.947162
2096.298213	199332.558722	37.952180
2098.348670	199592.511620	37.957197
2100.573151	199835.404299	37.962215
2103.278272	200077.980677	37.967232
2104.704658	200329.151028	37.972250
2106.941486	200569.074873	37.977268
2109.063339	200820.124495	37.982285
2111.087692	201059.551082	37.987303
2113.497846	201299.184084	37.992320
2115.556480	201542.821494	37.997338
2117.759337	201787.807987	38.002356
2119.914821	202024.298494	38.007373
2121.990888	202275.311226	38.012391
2124.221021	202512.147382	38.017408
2126.233971	202750.542211	38.022426
2128.186361	202959.930042	38.027444
2130.695333	203177.379718	38.032461
2132.074159	203388.383339	38.037479
2134.204972	203608.446078	38.042496
2136.287455	203828.301540	38.047514
2138.437516	204047.334726	38.052532
2140.184856	204268.742907	38.057549
2142.134283	204501.011310	38.062567
2144.517786	204728.984708	38.067584
2146.439923	204965.956095	38.072602
2148.696360	205186.017658	38.077620
2151.108291	205419.688923	38.082637
2152.946302	205664.064496	38.087655
2155.406137	205895.038894	38.092672
2157.211411	206131.183029	38.097690
2159.750536	206368.595425	38.102708
2161.877859	206616.458108	38.107725
2164.129847	206849.284502	38.112743
2166.585192	207084.275712	38.117760
2168.767486	207324.401666	38.122778
2171.162237	207557.893691	38.127796
2173.390725	207792.314309	38.132813
2175.529962	208019.983708	38.137831
2178.071856	208257.492027	38.142848
2180.032271	208498.305267	38.147866
2183.011410	208706.433692	38.152884
2185.213318	208944.684123	38.157901
2187.273000	209168.587343	38.162919
2189.654941	209390.866100	38.167936
2191.552228	209626.666554	38.172954
2193.839109	209846.676912	38.177972
2196.361856	210075.118303	38.182989
2198.491955	210299.776149	38.188007
2200.784865	210525.170698	38.193024
2203.009755	210745.270217	38.198042
2205.132282	210968.484390	38.203060
2207.780840	211197.316162	38.208077
2209.790236	211429.423952	38.213095
2212.154071	211634.904812	38.218112
2214.337384	211860.346874	38.223130
2216.702719	212079.260752	38.228148
2219.219110	212299.319418	38.233165
2221.332850	212518.807893	38.238183
2223.743697	212724.424428	38.243200
2225.741243	212947.449471	38.248218
2227.925251	213154.741074	38.253236
2230.698211	213380.894765	38.258253
2232.722011	213591.729882	38.263271
2235.259631	213788.823455	38.268288
2237.430037	214008.244454	38.273306
2239.436123	214216.164308	38.278324
2241.679960	214432.883523	38.283341
2243.619521	214646.338018	38.288359
2245.843940	214853.945925	38.293376
2247.654944	215064.692473	38.298394
2249.875907	215267.046010	38.303412
2252.022154	215450.520081	38.308429
2254.281402	215656.690259	38.313447
2256.280971	215843.096074	38.318464
2258.335066	216046.671829	38.323482
2260.356624	216253.465515	38.328500
2262.271145	216463.527060	38.333517
2264.326670	216673.808118	38.338535
2266.434477	216889.083922	38.343552
2268.221359	217123.735315	38.348570
2270.356266	217354.777292	38.353588
2272.968678	217593.654290	38.358605
2274.710034	217846.928482	38.363623
2277.109452	218078.235609	38.368640
2279.391627	218330.765561	38.373658
2281.627441	218577.539431	38.378676
2283.959144	218833.085124	38.383693
2286.052107	219085.685812	38.388711
2288.762476	219331.257010	38.393728
2290.676615	219593.677101	38.398746
2292.992476	219845.419786	38.403764
2295.404838	220108.143645	38.408781
2297.815700	220377.572720	38.413799
2300.058173	220637.824068	38.418816
2302.645627	220900.472186	38.423834
2304.781919	221156.488626	38.428852
2307.151385	221430.295887	38.433869
2309.344883	221692.044223	38.438887
2311.890591	221949.636394	38.443904
2313.971113	222225.536585	38.448922
2316.821822	222482.002922	38.453940
2319.072249	222758.779605	38.458957
2321.407444	223032.534531	38.463975
2324.031583	223292.023371	38.468992
2326.676344	223564.004221	38.474010
2328.856408	223862.838965	38.479028
2331.208273	224145.915181	38.484045
2333.189422	224408.214206	38.489063
2335.786655	224672.663938	38.494080
2338.124238	224950.132847	38.499098
2340.506793	225213.793020	38.504116
2342.990148	225474.492161	38.509133
2345.643728	225746.186949	38.514151
2348.162380	226006.577435	38.519168
2350.224321	226275.371020	38.524186
2352.537478	226540.976539	38.529204
2355.306922	226807.094692	38.534221
2357.311234	227081.664930	38.539239
2359.550853	227340.986358	38.544256
2361.843249	227617.722148	38.549274
2364.337295	227878.452479	38.554292
2366.855912	228139.459067	38.559309
2369.074111	228414.025072	38.564327
2371.507402	228670.323005	38.569344
2374.358703	228924.091948	38.574362
2376.601291	229167.519988	38.579380
2378.775536	229399.759483	38.584397
2380.901553	229638.991401	38.589415
2383.498307	229863.215881	38.594432
2385.426794	230111.724899	38.599450
2387.708039	230365.512104	38.604468
2390.007712	230594.560158	38.609485
2392.131244	230861.554922	38.614503
2394.240601	231107.650639	38.619520
2396.835062	231370.076901	38.624538
2398.866314	231634.167810	38.629556
2401.209017	231895.670344	38.634573
2403.384997	232171.473529	38.639591
2406.250491	232442.876022	38.644608
2408.221126	232720.414994	38.649626
2410.309310	232995.878907	38.654644
2413.005674	233276.022045	38.659661
2415.074846	233564.189580	38.664679
2417.636381	233854.057805	38.669696
2420.144720	234145.967169	38.674714
2422.690820	234440.030261	38.679732
2425.259088	234728.045897	38.684749
2427.758625	235024.784909	38.689767
2430.254098	235316.521928	38.694784
2432.737893	235613.544534	38.699802
2435.153581	235910.223208	38.704820
2437.881309	236198.573301	38.709837
2439.920448	236506.031601	38.714855
2442.416415	236807.373477	38.719872
2445.036287	237102.702425	38.724890
2447.468794	237400.474784	38.729908
2450.255778	237695.575689	38.734925
2452.534052	238004.956128	38.739943
2455.365941	238298.984786	38.744960
2457.824189	238598.635876	38.749978
2460.357790	238897.183660	38.754996
2463.081855	239188.158431	38.760013
2465.393867	239490.476612	38.765031
2468.140878	239783.684427	38.770048
2470.614013	240086.131044	38.775066
2472.692857	240379.827238	38.780084
2475.413526	240685.715944	38.785101
2477.667968	240989.444133	38.790119
2480.054222	241288.326234	38.795136
2482.782479	241588.577285	38.800154
2485.299831	241891.275495	38.805172
2488.194656	242193.457445	38.810189
2490.550249	242497.884583	38.815207
2493.138277	242792.394966	38.820224
2496.003719	243094.405955	38.825242
2498.223740	243395.275310	38.830260
2500.542667	243692.472048	38.835277
2503.356049	243986.187471	38.840295
2505.947873	244278.465432	38.845312
2508.143371	244565.548924	38.850330
2510.297541	244844.740003	38.855348
2513.203957	245106.489251	38.860365
2514.982794	245375.555244	38.865383
2516.956879	245650.483799	38.870400
2519.625413	245935.005976	38.875418
2521.817204	246211.831611	38.880436
2524.254333	246500.481132	38.885453
2526.758680	246794.784998	38.890471
2529.047089	247090.927149	38.895488
2531.825578	247393.494926	38.900506
2534.201180	247699.454699	38.905524
2536.853351	247993.077135	38.910541
2539.302976	248308.831270	38.915559
2541.428618	248617.067818	38.920576
2544.192695	248924.391000	38.925594
2546.467286	249245.077240	38.930612
2549.208517	249565.944221	38.935629
2551.551300	249899.016864	38.940647
2554.261889	250215.876572	38.945664
2557.000665	250544.467945	38.950682
2558.997029	250884.735310	38.955700
2562.067202	251208.042762	38.960717
2564.658225	251538.971039	38.965735
2567.482560	251875.095751	38.970752
2570.123337	252197.660227	38.975770
2572.678104	252534.413141	38.980788
2575.675735	252855.042537	38.985805
2577.964898	253196.385692	38.990823
2581.032567	253527.927997	38.995840
2583.751048	253850.660897	39.000858
2586.178839	254190.891606	39.005876
2588.952230	254514.328176	39.010893
2591.597146	254845.050643	39.015911
2594.220635	255182.076791	39.020928
2596.580511	255519.907320	39.025946
2599.553279	255852.814884	39.030964
2602.209843	256181.226047	39.035981
2604.523840	256510.682667	39.040999
2607.290479	256844.335686	39.046016
2610.359380	257171.336697	39.051034
2612.487129	257515.100467	39.056052
2615.338115	257839.342680	39.061069
2618.422910	258175.055654	39.066087
2620.296317	258506.261500	39.071104
2623.097121	258842.426823	39.076122
2625.551824	259184.921869	39.081140
2628.774966	259518.912780	39.086157
2631.402456	259862.930921	39.091175
2633.792057	260199.925226	39.096192
2636.579279	260523.368101	39.101210
2638.936735	260862.959390	39.106228
2641.676856	261198.553036	39.111245
2644.365339	261539.337428	39.116263
2646.571076	261875.854776	39.121280
2649.514593	262208.597621	39.126298
2651.711057	262528.046391	39.131316
2654.568839	262830.828010	39.136333
2656.923029	263150.252407	39.141351
2659.351913	263457.852879	39.146368
2661.949445	263773.835314	39.151386
2664.321169	264088.786863	39.156404
2666.896863	264416.128476	39.161421
2669.459409	264739.712798	39.166439
2672.050887	265073.936708	39.171456
2674.709055	265412.240236	39.176474
2677.372460	265758.951652	39.181492
2680.304981	266088.803827	39.186509
2682.730298	266445.638546	39.191527
2684.921111	266788.919959	39.196544
2687.848184	267136.047917	39.201562
2690.606041	267497.657354	39.206580
2693.198390	267852.485175	39.211597
2695.984845	268215.970402	39.216615
2698.384157	268585.156693	39.221632
2701.417686	268949.695576	39.226650
2703.884642	269318.490529	39.231668
2707.087888	269691.259013	39.236685
2709.684795	270060.338606	39.241703
2712.364014	270422.368605	39.246720
2715.180499	270792.912549	39.251738
2717.916130	271171.598523	39.256756
2720.316776	271550.667928	39.261773
2723.172511	271926.439163	39.266791
2725.688422	272306.786127	39.271808
2728.585683	272699.266437	39.276826
2731.307711	273087.125765	39.281844
2734.155410	273464.194222	39.286861
2737.009376	273863.769171	39.291879
2739.909832	274253.683511	39.296896
2742.873608	274635.966832	39.301914
2745.272383	275022.988463	39.306932
2748.538697	275408.145296	39.311949
2751.417414	275800.120803	39.316967
2754.322061	276184.191718	39.321984
2757.362281	276571.289539	39.327002
2760.061160	276963.268003	39.332020
2763.135399	277335.321503	39.337037
2766.083698	277719.359871	39.342055
2768.783489	278096.476965	39.347072
2771.811077	278466.327494	39.352090
2774.321337	278842.966314	39.357108
2777.255248	279226.676274	39.362125
2780.126284	279598.126220	39.367143
2782.538120	279978.971750	39.372160
2785.512513	280356.705042	39.377178
2788.215763	280732.347202	39.382196
2790.914458	281111.851193	39.387213
2793.732673	281493.088878	39.392231
2796.285937	281884.097740	39.397248
2799.175833	282247.033257	39.402266
2801.749084	282609.180371	39.407284
2804.487618	282955.678093	39.412301
2807.021872	283303.224055	39.417319
2809.597092	283661.381824	39.422336
2812.203136	284022.989277	39.427354
2814.657809	284394.959492	39.432372
2817.302630	284753.054584	39.437389
2820.116560	285129.793886	39.442407
2822.208576	285509.416065	39.447424
2825.241683	285901.641224	39.452442
2827.716795	286291.236191	39.457460
2830.646648	286686.118786	39.462477
2833.406963	287096.345770	39.467495
2836.245336	287497.948308	39.472512
2839.132953	287907.671492	39.477530
2841.728787	288320.742716	39.482548
2844.718178	288727.959239	39.487565
2847.889352	289140.328605	39.492583
2850.142039	289571.488418	39.497600
2853.660369	289982.734702	39.502618
2856.447840	290411.446104	39.507636
2859.177566	290841.969547	39.512653
2862.042172	291262.944948	39.517671
2864.836297	291702.525480	39.522688
2868.201232	292128.907173	39.527706
2870.838798	292574.226477	39.532724
2873.895790	293002.179494	39.537741
2877.014211	293437.361660	39.542759
2879.856021	293879.724815	39.547776
2883.219023	294312.148491	39.552794
2885.725021	294741.252242	39.557812
2889.075070	295179.137664	39.562829
2891.811190	295604.824700	39.567847
2894.869723	296045.624820	39.572864
2897.853745	296476.681372	39.577882
2900.552078	296922.337481	39.582900
2903.488232	297357.235296	39.587917
2906.741388	297787.941409	39.592935
2909.467323	298233.412154	39.597952
2912.493819	298668.292503	39.602970
2915.458169	299112.885017	39.607988
2918.575336	299552.168658	39.613005
2921.764833	299986.588013	39.618023
2924.352853	300428.544032	39.623040
2927.536604	300861.869698	39.628058
2930.312888	301300.034112	39.633076
2933.463035	301740.652842	39.638093
2936.355180	302188.906079	39.643111
2939.545324	302631.801999	39.648128
2942.673438	303063.555383	39.653146
2945.585511	303497.602364	39.658164
2948.339494	303930.072803	39.663181
2951.102548	304365.182164	39.668199
2954.080159	304807.368400	39.673216
2957.182620	305227.790550	39.678234
2959.787946	305637.139248	39.683252
2962.960479	306038.700596	39.688269
2965.754198	306423.454833	39.693287
2967.999567	306840.832479	39.698304
2971.187036	307240.127136	39.703322
2974.184331	307653.217499	39.708340
2977.020659	308059.016767	39.713357
2979.894080	308476.391212	39.718375
2982.557238	308893.467309	39.723392
2985.707808	309312.877812	39.728410
2988.631021	309755.385730	39.733428
2991.108497	310185.846921	39.738445
2994.122059	310608.855834	39.743463
2996.631956	311063.692135	39.748480
2999.552235	311508.530551	39.753498
3002.755826	311955.430503	39.758516
3005.245876	312418.671577	39.763533
3008.749082	312880.048636	39.768551
3011.366405	313347.456443	39.773568
3014.675086	313817.368874	39.778586
3017.602516	314301.537375	39.783604
3020.503353	314774.075313	39.788621
3024.232240	315240.816211	39.793639
3027.172146	315721.471078	39.798656
3030.212404	316194.996281	39.803674
3033.406805	316688.356100	39.808692
3036.328887	317151.837792	39.813709
3039.422075	317635.786211	39.818727
3042.480925	318126.112434	39.823744
3045.722782	318606.984684	39.828762
3048.928691	319095.428580	39.833780
3051.711345	319587.009940	39.838797
3055.234980	320065.798263	39.843815
3058.174943	320556.892360	39.848832
3061.378542	321046.189676	39.853850
3064.290041	321537.993991	39.858868
3067.429364	322033.365820	39.863885
3070.313026	322523.670596	39.868903
3073.530202	323027.989344	39.873920
3076.946510	323514.801070	39.878938
3079.981231	324008.603456	39.883956
3082.579601	324515.195259	39.888973
3086.458501	325001.391810	39.893991
3089.351173	325503.181970	39.899008
3092.645870	326003.686439	39.904026
3095.748726	326498.326449	39.909044
3098.923228	326998.056443	39.914061
3102.336386	327485.048068	39.919079
3104.904497	327987.407163	39.924096
3107.991580	328483.205276	39.929114
3111.035188	328982.892389	39.934132
3114.180728	329480.680908	39.939149
3117.686809	329970.536932	39.944167
3120.524290	330478.652118	39.949184
3123.716469	330974.518714	39.954202
3126.945801	331434.291857	39.959220
3129.615466	331895.242532	39.964237
3132.494996	332349.478635	39.969255
3135.356828	332815.573194	39.974272
3138.351497	333290.048708	39.979290
3141.613518	333758.587611	39.984308
3144.092200	334242.736714	39.989325
3147.376308	334715.683945	39.994343
3150.318007	335204.349042	39.999360
3153.455771	335713.547110	40.004378
3156.703882	336206.269991	40.009396
3159.614648	336705.745979	40.014413
3162.734252	337205.794557	40.019431
3165.397562	337728.382724	40.024448
3168.724259	338228.644634	40.029466
3171.898004	338752.438751	40.034484
3174.753663	339283.870686	40.039501
3178.065949	339806.974075	40.044519
3181.103865	340353.678592	40.049536
3184.379029	340894.374165	40.054554
3187.558612	341429.392841	40.059572
3190.727695	341988.604707	40.064589
3194.150583	342524.286235	40.069607
3197.337785	343082.037976	40.074624
3200.709690	343621.805438	40.079642
3204.304678	344175.217155	40.084660
3207.562872	344730.631852	40.089677
3211.413498	345256.700504	40.094695
3215.290278	345806.091698	40.099712
3218.406088	346339.756139	40.104730
3221.568614	346883.740877	40.109748
3224.730248	347416.017077	40.114765
3228.227716	347961.283999	40.119783
3231.242499	348507.256610	40.124800
3234.825028	349045.721236	40.129818
3238.387305	349584.259963	40.134836
3241.380453	350131.996932	40.139853
3244.962213	350667.044015	40.144871
3247.824245	351203.341955	40.149888
3251.266990	351752.133709	40.154906
3254.734650	352282.156443	40.159924
3258.054273	352821.868804	40.164941
3261.173731	353367.344127	40.169959
3264.732451	353909.901252	40.174976
3267.640140	354449.941105	40.179994
3271.100483	354996.766824	40.185012
3273.826445	355549.870946	40.190029
3277.390348	356085.753766	40.195047
3280.940462	356635.771234	40.200064
3284.120283	357184.876671	40.205082
3287.218847	357729.724680	40.210100
3290.531215	358289.914275	40.215117
3294.294275	358822.487174	40.220135
3297.415817	359381.273050	40.225152
3300.323939	359911.786384	40.230170
3303.643462	360416.441968	40.235188
3306.479364	360929.087400	40.240205
3309.655805	361436.572026	40.245223
3312.867128	361951.634278	40.250240
3316.160397	362460.764456	40.255258
3319.146429	362983.845551	40.260276
3322.438855	363513.978437	40.265293
3325.699639	364046.952649	40.270311
3328.740003	364586.071725	40.275328
3331.946832	365121.884308	40.280346
3335.096081	365655.847064	40.285364
3337.988200	366208.192122	40.290381
3341.259198	366762.754404	40.295399
3344.869721	367329.563894	40.300416
3348.166813	367896.390286	40.305434
3351.336070	368465.386552	40.310452
3355.036424	369042.944620	40.315469
3358.370328	369621.644079	40.320487
3361.513141	370200.315225	40.325504
3364.750730	370792.615266	40.330522
3368.575061	371371.467283	40.335540
3371.824652	371957.177154	40.340557
3375.368543	372558.411877	40.345575
3378.689790	373155.867124	40.350592
3382.138171	373751.898153	40.355610
3385.576436	374344.547596	40.360628
3388.926854	374955.419727	40.365645
3392.595253	375553.546440	40.370663
3395.857188	376166.773947	40.375680
3399.637625	376771.461531	40.380698
3403.494225	377362.757503	40.385716
3406.482852	377983.180342	40.390733
3410.103817	378586.698510	40.395751
3413.788708	379179.643522	40.400768
3417.152940	379796.528102	40.405786
3420.772962	380387.486193	40.410804
3424.204091	380996.349899	40.415821
3427.752545	381597.346670	40.420839
3431.163380	382217.762023	40.425856
3434.601439	382824.109471	40.430874
3438.129547	383424.319534	40.435892
3441.646772	384027.337402	40.440909
3445.288708	384632.076079	40.445927
3449.161704	385250.338999	40.450944
3452.475008	385842.097294	40.455962
3456.404123	386442.956142	40.460980
3459.986179	387053.549160	40.465997
3463.346815	387630.001650	40.471015
3466.754514	388232.764888	40.476032
3470.169497	388833.437091	40.481050
3474.361418	389427.508912	40.486068
3477.377802	390021.731250	40.491085
3480.994717	390612.500927	40.496103
3484.364468	391206.824994	40.501120
3487.686930	391779.009796	40.506125
3491.175752	392308.710303	40.511130
3493.859942	392814.096364	40.516135
3496.952623	393251.195809	40.521140
3499.585160	393640.793206	40.526144
3502.068987	393976.408597	40.531149
3504.578507	394259.922800	40.536154
3507.176257	394492.445873	40.541159
3509.387032	394665.537007	40.546164
3510.913958	394810.820197	40.551168
3512.251399	394906.429682	40.556173
3513.799630	394961.455088	40.561178
3514.441070	394997.174749	40.566183
3515.666962	394998.836232	40.571188
3516.539792	394967.172451	40.576192
3516.771351	394920.050779	40.581197
3517.512411	394838.908010	40.586202
3517.931007	394757.536352	40.591207
3518.251598	394653.730822	40.596212
3518.876735	394534.419153	40.601216
3518.710907	394407.579470	40.606221
3519.136250	394260.484622	40.611226
3518.998576	394111.800128	40.616231
3518.931332	393956.061334	40.621236
3519.172726	393779.247080	40.626240
3519.037427	393609.305222	40.631245
3519.271097	393432.210731	40.636250
3519.042778	393251.832270	40.641255
3518.801507	393067.742872	40.646260
3518.360043	392879.183895	40.651264
3518.131080	392692.217517	40.656269
3518.061463	392509.801506	40.661274
3517.642995	392335.601245	40.666279
3517.302631	392151.548060	40.671284
3517.045794	391965.192383	40.676288
3516.638540	391797.344086	40.681293
3516.481577	391619.869827	40.686298
3515.867834	391465.299505	40.691303
3515.509291	391288.618205	40.696308
3515.349303	391130.237034	40.701312
3515.160286	390976.105953	40.706317
3515.068224	390808.152244	40.711322
3514.527614	390669.560168	40.716327
3514.299477	390516.679164	40.721332
3514.206598	390365.733991	40.726336
3513.786917	390228.087290	40.731341
3513.700567	390083.649191	40.736346
3513.271244	389953.046249	40.741351
3513.017435	389822.669359	40.746356
3512.616297	389687.840056	40.751360
3512.253893	389559.284705	40.756365
3512.391797	389431.412646	40.761370
3512.038837	389318.823442	40.766375
3511.836952	389208.167941	40.771380
3511.674988	389086.851536	40.776384
3511.339327	388965.714738	40.781389
3511.107414	388862.716708	40.786394
3510.889596	388764.852620	40.791399
3510.632975	388651.991808	40.796404
3510.852484	388560.669354	40.801408
3510.485610	388460.971736	40.806413
3510.372560	388361.411723	40.811418
3510.070510	388281.435738	40.816423
3509.662567	388183.422113	40.821428
3509.623401	388093.639635	40.826432
3509.326749	388019.993916	40.831437
3509.548889	387931.619163	40.836442
3509.072625	387853.246336	40.841447
3509.125463	387769.119106	40.846452
3508.886630	387701.210493	40.851456
3508.792136	387632.821222	40.856461
3508.888302	387551.788956	40.861466
3508.307222	387489.070674	40.866471
3508.150178	387422.114910	40.871476
3508.401851	387350.796919	40.876480
3508.111207	387291.389025	40.881485
3508.039238	387227.343800	40.886490
3508.119727	387170.063955	40.891495
3508.133677	387106.386375	40.896500
3507.898155	387036.619662	40.901504
3507.680587	386988.210589	40.906509
3507.638427	386923.778679	40.911514
3507.431079	386876.283299	40.916519
3507.064117	386824.668090	40.921524
3507.167022	386776.309803	40.926528
3507.368176	386732.970959	40.931533
3507.597745	386672.437226	40.936538
3507.208691	386632.853395	40.941543
3506.977166	386579.105780	40.946548
3506.770038	386534.432603	40.951552
3506.883008	386491.005691	40.956557
3506.962627	386434.411427	40.961562
3506.842046	386400.506590	40.966567
3506.842952	386357.224379	40.971572
3506.663225	386301.306642	40.976576
3506.749996	386259.104225	40.981581
3506.692146	386224.121258	40.986586
3506.313602	386181.229398	40.991591
3506.432044	386145.277588	40.996596
3506.469270	386120.120857	41.001600
3505.824614	386088.790690	41.006605
3506.394933	386046.765904	41.011610
3506.303583	386014.610755	41.016615
3506.012862	385983.707728	41.021620
3506.514116	385944.160449	41.026624
3506.253669	385909.641513	41.031629
3506.074220	385870.964641	41.036634
3506.025239	385846.507959	41.041639
3506.166566	385812.459463	41.046644
3506.020996	385771.641002	41.051648
3505.863626	385745.548425	41.056653
3506.234862	385710.013978	41.061658
3505.982698	385677.451638	41.066663
3506.269320	385647.143696	41.071668
3505.874453	385605.652406	41.076672
3505.723163	385585.484003	41.081677
3505.816113	385561.665887	41.086682
3505.790321	385541.808219	41.091687
3505.518002	385510.774734	41.096692
3505.646789	385486.264287	41.101696
3505.070559	385457.847255	41.106701
3505.386133	385437.274388	41.111706
3505.363651	385414.923953	41.116711
3505.394637	385395.438688	41.121716
3505.423175	385366.417394	41.126720
3505.524848	385346.412323	41.131725
3505.746539	385320.513839	41.136730
3505.283478	385302.886740	41.141735
3505.310785	385270.686758	41.146740
3505.321074	385244.719911	41.151744
3504.934116	385232.243142	41.156749
3505.271413	385212.811090	41.161754
3505.331451	385200.390816	41.166759
3505.217946	385176.579651	41.171764
3505.191019	385147.719535	41.176768
3505.327728	385136.431497	41.181773
3505.462287	385106.960923	41.186778
3505.313347	385095.845173	41.191783
3505.240328	385076.910221	41.196788
3505.403790	385047.791060	41.201792
3504.964519	385040.790081	41.206797
3505.304438	385013.601164	41.211802
3505.056520	384991.006365	41.216807
3504.980909	384977.259629	41.221812
3505.319206	384954.419573	41.226816
3504.918793	384945.301686	41.231821
3505.551351	384912.395395	41.236826
3504.878355	384901.311551	41.241831
3504.822501	384882.856971	41.246836
3505.199602	384855.458616	41.251840
3504.971977	384846.262534	41.256845
3505.202550	384825.194147	41.261850
3505.107874	384811.323209	41.266855
3504.894856	384785.671072	41.271860
3505.196145	384774.128035	41.276864
3504.988300	384758.927130	41.281869
3505.269477	384728.034386	41.286874
3505.104508	384722.286967	41.291879
3505.327890	384697.608462	41.296884
3505.370133	384674.942179	41.301888
3504.951361	384658.325009	41.306893
3504.998068	384635.200240	41.311898
3504.932579	384615.577228	41.316903
3504.768231	384615.195620	41.321908
3504.822232	384594.892507	41.326912
3504.566590	384581.479250	41.331917
3504.919621	384559.018086	41.336922
3504.853521	384551.042519	41.341927
3504.643827	384529.814670	41.346932
3504.947075	384519.085036	41.351936
3504.505379	384508.193396	41.356941
3504.902883	384501.594114	41.361946
3504.803814	384484.290561	41.366951
3504.965600	384475.999220	41.371956
3504.762076	384452.990180	41.376960
3504.757269	384435.391965	41.381965
3504.888751	384420.671343	41.386970
3504.811163	384415.596704	41.391975
3504.778879	384392.331683	41.396980
3504.953613	384385.233536	41.401984
3504.662500	384369.435285	41.406989
3504.497241	384349.624453	41.411994
3504.351602	384337.923037	41.416999
3504.501525	384321.749888	41.422004
3504.754272	384323.209690	41.427008
3504.305822	384314.353551	41.432013
3504.722310	384294.755917	41.437018
3504.746770	384290.834966	41.442023
3504.953937	384268.650993	41.447028
3504.992879	384249.723355	41.452032
3504.806449	384231.085640	41.457037
3504.681081	384218.312873	41.462042
3504.184773	384213.228091	41.467047
3504.363219	384206.180186	41.472052
3504.419232	384183.460566	41.477056
3504.271878	384187.603026	41.482061
3504.467422	384174.830387	41.487066
3504.450552	384180.554392	41.492071
3504.493213	384176.172790	41.497076
3504.978018	384157.123775	41.502080
3504.717226	384147.729311	41.507085
3504.663242	384122.026151	41.512090
3504.662121	384115.871272	41.517095
3504.909478	384094.596370	41.522100
3504.745601	384087.195646	41.527104
3504.711876	384071.788921	41.532109
3504.935838	384056.951814	41.537114
3504.774298	384029.612553	41.542119
3504.200423	384022.861537	41.547124
3504.435076	384010.743875	41.552128
3504.224547	384002.765587	41.557133
3504.437769	383997.263459	41.562138
3504.608514	383998.100451	41.567143
3504.337622	383978.153528	41.572148
3504.641941	383963.278252	41.577152
3504.403265	383962.628640	41.582157
3504.692679	383948.264341	41.587162
3504.616648	383947.767042	41.592167
3504.595799	383922.312821	41.597172
3504.587205	383909.190884	41.602176
3504.513015	383894.553424	41.607181
3504.751160	383889.759421	41.612186
3504.523721	383870.822830	41.617191
3504.777886	383856.260616	41.622196
3504.840616	383841.652358	41.627200
3504.537593	383836.333524	41.632205
3504.831063	383810.778687	41.637210
3504.787975	383802.621302	41.642215
3504.313033	383781.562107	41.647220
3504.555729	383772.393151	41.652224
3504.345710	383768.687225	41.657229
3504.280936	383755.548682	41.662234
3504.030700	383746.559354	41.667239
3504.368169	383738.214651	41.672244
3504.720925	383742.023803	41.677248
3504.270435	383734.998918	41.682253
3504.401165	383723.940281	41.687258
3504.662000	383707.469590	41.692263
3504.595759	383700.968894	41.697268
3504.602114	383685.377654	41.702272
3504.586286	383670.603725	41.707277
3504.604632	383667.116011	41.712282
3504.500236	383646.532239	41.717287
3504.343261	383637.502713	41.722292
3504.753448	383625.560636	41.727296
3504.265785	383623.144726	41.732301
3504.502775	383606.855781	41.737306
3504.479635	383589.285497	41.742311
3504.352505	383579.183111	41.747316
3504.121198	383579.981930	41.752320
3504.194929	383563.210136	41.757325
3504.325280	383548.311329	41.762330
3504.564917	383557.021256	41.767335
3504.397291	383537.642705	41.772340
3504.628894	383516.904030	41.777344
3504.592278	383522.275214	41.782349
3504.530086	383505.855488	41.787354
3504.527360	383500.870620	41.792359
3504.407025	383481.103090	41.797364
3504.370524	383468.010841	41.802368
3504.519626	383468.215473	41.807373
3504.450714	383441.166324	41.812378
3504.435540	383441.168034	41.817383
3504.354102	383433.728719	41.822388
3504.564861	383412.408351	41.827392
3504.083627	383416.018736	41.832397
3504.700058	383405.646193	41.837402
3504.713873	383386.950977	41.842407
3504.347117	383377.293318	41.847412
3504.252346	383359.785111	41.852416
3504.241953	383350.020259	41.857421
3504.560720	383335.956269	41.862426
3504.457679	383329.715643	41.867431
3504.334902	383324.368248	41.872436
3504.457565	383314.811243	41.877440
3504.534240	383301.777344	41.882445
3504.675588	383291.657880	41.887450
3504.341483	383285.504630	41.892455
3504.116331	383268.779943	41.897460
3504.468742	383268.698125	41.902464
3504.274599	383247.874000	41.907469
3504.638246	383238.965548	41.912474
3504.378633	383242.922400	41.917479
3504.584054	383223.382999	41.922484
3504.507359	383210.017262	41.927488
3504.285218	383206.389492	41.932493
3504.384335	383178.270889	41.937498
3504.296911	383184.947178	41.942503
3504.247063	383170.636203	41.947508
3504.446038	383151.402967	41.952512
3504.197537	383160.597048	41.957517
3504.434194	383147.334355	41.962522
3504.288164	383134.335597	41.967527
3504.353858	383119.650294	41.972532
3504.304694	383114.392963	41.977536
3504.236709	383097.923111	41.982541
3504.110051	383099.086880	41.987546
3504.216207	383096.882266	41.992551
3504.098131	383078.106013	41.997556
3504.457302	383071.563404	42.002560
3504.552138	383072.005503	42.007565
3504.650910	383049.456462	42.012570
3504.140789	383043.229263	42.017575
3504.273845	383036.213745	42.022580
3504.643653	383021.124291	42.027584
3504.383789	383006.541263	42.032589
3504.567106	383000.941988	42.037594
3504.337180	382989.558657	42.042599
3504.405251	382972.533174	42.047604
3504.466162	382955.635976	42.052608
3503.897062	382959.311154	42.057613
3504.344245	382941.132160	42.062618
3504.171092	382955.985733	42.067623
3504.214032	382936.675320	42.072628
3504.130940	382921.021605	42.077632
3504.228917	382925.532343	42.082637
3504.242957	382914.695369	42.087642
3504.266339	382897.270002	42.092647
3504.212620	382893.869903	42.097652
3504.318279	382884.849551	42.102656
3504.237268	382875.502650	42.107661
3504.315876	382862.061380	42.112666
3504.510665	382856.740024	42.117671
3504.182083	382842.218657	42.122676
3504.164009	382833.370442	42.127680
3504.181646	382837.893888	42.132685
3504.433853	382828.189124	42.137690
3504.298340	382822.589350	42.142695
3504.280947	382810.816324	42.147700
3504.527931	382803.350410	42.152704
3504.335755	382791.528706	42.157709
3504.562845	382783.302967	42.162714
3504.293937	382766.025465	42.167719
3504.507162	382759.887351	42.172724
3504.615796	382758.343563	42.177728
3504.476108	382730.058912	42.182733
3504.797894	382708.898624	42.187738
3504.450431	382706.587656	42.192743
3504.328189	382694.754869	42.197748
3504.513977	382681.627214	42.202752
3504.110712	382668.007712	42.207757
3504.347877	382647.038791	42.212762
3503.944671	382653.510760	42.217767
3504.312943	382648.314550	42.222772
3504.456137	382632.243467	42.227776
3504.202323	382626.153715	42.232781
3504.599540	382610.525688	42.237786
3504.493861	382602.606827	42.242791
3504.298049	382598.186435	42.247796
3504.100004	382563.095025	42.252800
3503.743270	382569.788556	42.257805
3504.572746	382562.662881	42.262810
3504.365534	382557.226993	42.267815
3504.292630	382545.055741	42.272820
3504.270974	382530.282286	42.277824
3504.416927	382530.843474	42.282829
3504.468079	382507.920152	42.287834
3504.186905	382505.446100	42.292839
3504.313092	382503.161988	42.297844
3504.598716	382471.834337	42.302848
3504.015205	382477.164944	42.307853
3504.203531	382462.714328	42.312858
3504.112582	382458.964021	42.317863
3504.079076	382449.533210	42.322868
3504.042002	382437.941206	42.327872
3504.488706	382453.281952	42.332877
3504.369147	382428.554430	42.337882
3504.275543	382416.844192	42.342887
3504.266234	382413.004680	42.347892
3504.478278	382400.457724	42.352896
3504.090422	382388.717686	42.357901
3504.194134	382370.033191	42.362906
3504.046925	382375.218557	42.367911
3504.162945	382356.176055	42.372916
3504.382383	382352.605573	42.377920
3503.979728	382355.720420	42.382925
3504.236434	382336.045294	42.387930
3504.304706	382328.175180	42.392935
3504.150991	382326.189621	42.397940
3504.407480	382325.131096	42.402944
3503.786087	382315.335382	42.407949
3504.105578	382296.387854	42.412954
3504.074680	382294.357450	42.417959
3503.824706	382295.693328	42.422964
3504.102147	382290.638588	42.427968
3503.957799	382280.767468	42.432973
3504.341030	382264.887184	42.437978
3504.128348	382273.414573	42.442983
3504.097353	382264.593699	42.447988
3504.375759	382247.356619	42.452992
3504.007051	382232.459872	42.457997
3503.970265	382232.414134	42.463002
3504.013307	382240.697652	42.468007
3503.835343	382224.371965	42.473012
3503.764410	382211.106694	42.478016
3503.726535	382218.385704	42.483021
3503.771378	382217.004571	42.488026
3503.973751	382219.108233	42.493031
3503.680089	382226.097045	42.498036
3504.247314	382212.705482	42.503040
3504.033072	382214.137446	42.508045
3504.217911	382191.726887	42.513050
3504.354800	382190.254907	42.518055
3504.279925	382182.331090	42.523060
3504.299541	382175.028151	42.528064
3504.096763	382168.548771	42.533069
3504.168292	382162.051467	42.538074
3504.152269	382146.310534	42.543079
3504.198754	382136.765272	42.548084
3504.289015	382133.418647	42.553088
3503.908619	382143.167904	42.558093
3504.170774	382119.651482	42.563098
3503.978538	382109.813319	42.568103
3504.254908	382105.750595	42.573108
3504.405739	382106.489048	42.578112
3504.133398	382090.000191	42.583117
3504.330661	382073.360808	42.588122
3504.410594	382073.678111	42.593127
3504.110358	382049.004331	42.598132
3504.036883	382037.697717	42.603136
3504.308831	382038.442461	42.608141
3504.144740	382030.736174	42.613146
3504.005603	382018.015702	42.618151
3503.675710	382002.960134	42.623156
3503.825946	382002.706807	42.628160
3503.845590	382014.910708	42.633165
3504.047588	382009.384633	42.638170
3504.143324	382003.417563	42.643175
3504.075379	381988.778377	42.648180
3504.436537	381984.269884	42.653184
3504.442939	381978.698421	42.658189
3504.049739	381957.396392	42.663194
3504.315151	381956.692505	42.668199
3504.015743	381942.115317	42.673204
3504.292167	381940.494110	42.678208
3503.973817	381933.804061	42.683213
3504.143130	381912.845459	42.688218
3504.382323	381920.335062	42.693223
3504.166941	381904.574672	42.698228
3504.298269	381887.564138	42.703232
3503.994116	381888.374505	42.708237
3503.964853	381882.605202	42.713242
3503.769132	381879.939573	42.718247
3503.780671	381869.738516	42.723252
3503.843749	381867.845832	42.728256
3503.903573	381870.251804	42.733261
3503.863568	381858.685519	42.738266
3503.966977	381865.687939	42.743271
3503.914777	381877.013091	42.748276
3503.813122	381851.646544	42.753280
3503.966440	381844.831067	42.758285
3504.032611	381831.315099	42.763290
3504.196255	381836.604005	42.768295
3504.394645	381836.546529	42.773300
3504.331457	381816.591068	42.778304
3504.056245	381810.758895	42.783309
3504.153384	381803.926856	42.788314
3503.845804	381797.947200	42.793319
3503.795023	381783.788446	42.798324
3504.098733	381773.617484	42.803329
3504.029278	381782.707300	42.808333
3504.395063	381778.757575	42.813338
3504.050364	381770.367660	42.818343
3503.929285	381749.836358	42.823348
3504.108727	381752.630358	42.828353
3504.058757	381751.747417	42.833357
3504.193646	381738.169690	42.838362
3503.904265	381729.211501	42.843367
3503.996754	381729.425091	42.848372
3504.182075	381719.527154	42.853377
3504.238388	381724.731308	42.858381
3504.451050	381705.571475	42.863386
3504.163021	381702.132004	42.868391
3503.863912	381690.886381	42.873396
3504.431705	381683.573008	42.878401
3504.382239	381678.773318	42.883405
3504.181464	381659.170147	42.888410
3504.368624	381654.053293	42.893415
3504.068485	381633.016137	42.898420
3503.980194	381639.743700	42.903425
3503.876896	381635.155976	42.908429
3504.508469	381623.280014	42.913434
3504.314455	381600.369461	42.918439
3504.082983	381588.807923	42.923444
3504.209254	381576.935510	42.928449
3503.947037	381579.163502	42.933453
3504.056578	381560.477689	42.938458
3503.978265	381560.285915	42.943463
3503.982340	381556.978294	42.948468
3504.081342	381553.630236	42.953473
3504.060791	381544.120854	42.958477
3504.176290	381532.173831	42.963482
3504.073226	381530.383689	42.968487
3503.925178	381521.072483	42.973492
3504.139072	381505.091483	42.978497
3504.051957	381500.577484	42.983501
3504.126728	381491.688849	42.988506
3504.433398	381497.845354	42.993511
3504.030671	381480.257787	42.998516
3504.227669	381460.235584	43.003521
3503.941156	381469.003718	43.008525
3504.599324	381459.717673	43.013530
3504.303967	381447.199733	43.018535
3504.138139	381431.405882	43.023540
3504.543751	381424.499589	43.028545
3504.139163	381415.406935	43.033549
3504.265059	381402.212007	43.038554
3504.151220	381391.521976	43.043559
3503.990348	381385.875131	43.048564
3504.041779	381370.097783	43.053569
3503.893720	381378.462559	43.058573
3504.130685	381372.930866	43.063578
3503.721485	381373.350916	43.068583
3503.757289	381380.618440	43.073588
3504.048979	381354.604434	43.078593
3503.922913	381347.934757	43.083597
3504.172675	381343.825293	43.088602
3504.139232	381350.696837	43.093607
3503.838360	381342.121870	43.098612
3504.063922	381329.903057	43.103617
3503.863864	381319.302931	43.108621
3504.183194	381308.798746	43.113626
3504.266350	381313.693515	43.118631
3504.088592	381317.866527	43.123636
3504.106293	381285.715521	43.128641
3503.857175	381282.600492	43.133645
3504.066542	381281.676553	43.138650
3503.867061	381284.708508	43.143655
3503.943668	381278.083086	43.148660
3503.889528	381257.032276	43.153665
3503.772462	381258.169151	43.158669
3504.305983	381248.546692	43.163674
3503.989868	381253.606306	43.168679
3503.864510	381251.539909	43.173684
3504.280594	381226.243718	43.178689
3504.145262	381230.460900	43.183693
3504.081754	381223.603282	43.188698
3504.129229	381218.864512	43.193703
3503.849973	381212.854854	43.198708
3503.764982	381194.403074	43.203713
3503.794968	381202.917780	43.208717
3504.133044	381193.020998	43.213722
3504.135773	381189.230326	43.218727
3503.879112	381192.500225	43.223732
3503.939121	381163.725051	43.228737
3503.955523	381162.551841	43.233741
3504.092110	381158.383945	43.238746
3504.045040	381163.197582	43.243751
3504.352215	381149.668717	43.248756
3504.329539	381138.964207	43.253761
3503.948164	381145.153214	43.258765
3504.064630	381133.002448	43.263770
3504.144001	381117.144281	43.268775
3503.840309	381109.688771	43.273780
3503.707450	381096.916134	43.278785
3503.801942	381099.138642	43.283789
3504.100135	381102.371720	43.288794
3503.743448	381106.471301	43.293799
3503.922798	381082.916462	43.298804
3504.327253	381065.150263	43.303809
3503.939023	381073.527630	43.308813
3504.192757	381061.507746	43.313818
3504.414006	381049.518426	43.318823
3503.813063	381042.160750	43.323828
3504.009506	381029.285177	43.328833
3504.116051	381032.167051	43.333837
3504.248378	381027.516581	43.338842
3504.267158	381011.388180	43.343847
3503.706342	381004.405655	43.348852
3503.852845	381004.763313	43.353857
3503.657493	381014.152977	43.358861
3503.681519	381003.949715	43.363866
3503.634644	381012.883545	43.368871
3503.730068	381002.974198	43.373876
3503.570527	380985.220801	43.378881
3503.883955	380976.090860	43.383885
3503.813743	380974.346366	43.388890
3503.834448	380974.851074	43.393895
3503.824639	380977.446141	43.398900
3504.148868	380981.590717	43.403905
3503.887549	380971.737746	43.408909
3503.979230	380954.885664	43.413914
3503.986841	380950.636397	43.418919
3503.830514	380948.193377	43.423924
3503.848866	380959.202449	43.428929
3504.001467	380971.131335	43.433933
3503.857979	380959.326800	43.438938
3503.928428	380936.806420	43.443943
3503.716560	380933.380274	43.448948
3503.920388	380925.081513	43.453953
3503.887056	380929.893008	43.458957
3503.870135	380932.540069	43.463962
3503.964591	380932.295552	43.468967
3503.754520	380922.994004	43.473972
3504.159629	380907.389468	43.478977
3503.706150	380908.681258	43.483981
3504.108635	380910.295563	43.488986
3504.134480	380908.688485	43.493991
3503.884716	380898.986269	43.498996
3504.005007	380872.210590	43.504001
3503.882075	380877.188854	43.509005
3504.260660	380864.564207	43.514010
3504.109818	380873.361901	43.519015
3503.785199	380862.298100	43.524020
3503.872379	380843.437439	43.529025
3503.879079	380844.351297	43.534029
3504.036191	380831.787076	43.539034
3503.636950	380844.235589	43.544039
3503.662833	380841.941798	43.549044
3503.939101	380838.031559	43.554049
3503.751608	380838.035071	43.559053
3503.733919	380816.622190	43.564058
3503.906208	380808.811625	43.569063
3504.074612	380811.302236	43.574068
3503.988216	380806.330239	43.579073
3504.002327	380816.195515	43.584077
3504.155166	380805.692073	43.589082
3503.945052	380792.041373	43.594087
3503.910390	380790.036916	43.599092
3504.315080	380778.221987	43.604097
3503.663545	380787.607505	43.609101
3503.777795	380775.660444	43.614106
3503.579635	380762.185878	43.619111
3503.767004	380752.338236	43.624116
3503.885504	380742.781245	43.629121
3503.941326	380752.512777	43.634125
3503.836594	380745.051184	43.639130
3503.970676	380751.616590	43.644135
3503.797730	380743.453639	43.649140
3504.159634	380730.246613	43.654145
3503.753495	380731.073122	43.659149
3503.804140	380719.008929	43.664154
3503.962831	380725.494148	43.669159
3503.861073	380725.509543	43.674164
3504.092074	380711.356725	43.679169
3503.704309	380704.524830	43.684173
3503.833810	380689.650473	43.689178
3503.983704	380691.177542	43.694183
3503.634345	380691.740742	43.699188
3503.813134	380682.911781	43.704193
3503.637063	380695.248769	43.709197
3503.818436	380691.963919	43.714202
3503.807633	380693.541820	43.719207
3503.985489	380669.096790	43.724212
3503.986347	380651.114419	43.729217
3503.625527	380658.953438	43.734221
3503.886685	380662.802813	43.739226
3503.729996	380662.801457	43.744231
3503.893522	380665.114814	43.749236
3504.279037	380652.082065	43.754241
3503.686222	380644.392391	43.759245
3504.159331	380626.030166	43.764250
3504.071688	380636.191340	43.769255
3503.965196	380633.918458	43.774260
3504.107316	380622.628219	43.779265
3503.868160	380612.619052	43.784269
3504.195900	380598.832407	43.789274
3504.112628	380604.262243	43.794279
3503.732999	380607.805962	43.799284
3503.986237	380585.816027	43.804289
3503.890999	380577.844229	43.809293
3504.271488	380570.534816	43.814298
3503.953749	380567.964681	43.819303
3503.920155	380565.603973	43.824308
3504.216608	380551.923991	43.829313
3504.081109	380546.934288	43.834317
3503.896648	380540.451736	43.839322
3504.001753	380535.424003	43.844327
3503.785890	380528.590341	43.849332
3503.851974	380512.683158	43.854337
3503.873663	380512.958813	43.859341
3503.924306	380495.222838	43.864346
3503.535753	380507.873239	43.869351
3503.983679	380506.224868	43.874356
3504.093755	380505.647242	43.879361
3503.771938	380506.104356	43.884365
3503.987138	380482.467184	43.889370
3503.909185	380477.315774	43.894375
3503.724428	380476.326939	43.899380
3503.853784	380476.178638	43.904385
3503.970191	380481.144559	43.909389
3504.185861	380463.102716	43.914394
3504.203519	380457.503819	43.919399
3503.804313	380447.825109	43.924404
3503.908757	380438.753505	43.929409
3503.669921	380446.547854	43.934413
3503.897643	380447.452223	43.939418
3504.031024	380444.988816	43.944423
3504.042970	380433.541060	43.949428
3504.026195	380424.615780	43.954433
3504.013767	380428.025178	43.959437
3503.979964	380427.241387	43.964442
3504.097993	380403.263452	43.969447
3504.089766	380390.216545	43.974452
3504.044688	380383.813672	43.979457
3503.832937	380389.670785	43.984461
3503.934667	380389.755753	43.989466
3503.909206	380370.658326	43.994471
3503.979419	380357.955083	43.999476
3503.900401	380355.677843	44.004481
3503.998416	380356.348377	44.009485
3504.081022	380351.985455	44.014490
3503.600005	380352.747504	44.019495
3503.580614	380332.021336	44.024500
3503.865823	380315.825101	44.029505
3503.400608	380322.917673	44.034509
3503.546341	380326.963362	44.039514
3503.880801	380317.499303	44.044519
3503.836128	380322.465269	44.049524
3504.337015	380321.927608	44.054529
3503.910269	380330.641862	44.059533
3504.187916	380318.338196	44.064538
3504.051260	380302.488404	44.069543
3503.722333	380299.843717	44.074548
3504.009865	380291.480723	44.079553
3503.474577	380305.731279	44.084557
3503.656040	380301.047522	44.089562
3503.942594	380304.257074	44.094567
3503.706356	380284.150130	44.099572
3503.884292	380275.982491	44.104577
3503.726079	380274.506212	44.109581
3504.023626	380258.536908	44.114586
3503.861202	380269.116939	44.119591
3503.707613	380259.373928	44.124596
3503.919111	380258.373327	44.129601
3503.883335	380259.319346	44.134605
3503.869106	380241.491773	44.139610
3503.728729	380239.478562	44.144615
3503.874917	380236.529875	44.149620
3503.973671	380223.466003	44.154625
3503.944584	380234.457345	44.159629
3503.709201	380228.822107	44.164634
3503.721293	380224.088807	44.169639
3503.535446	380212.138135	44.174644
3503.631817	380199.532442	44.179649
3503.541177	380203.513766	44.184653
3503.834888	380204.077071	44.189658
3503.814622	380203.596343	44.194663
3503.693272	380205.547810	44.199668
3503.929579	380201.643823	44.204673
3503.596656	380208.206829	44.209677
3503.826994	380202.625149	44.214682
3503.824566	380207.279246	44.219687
3503.868377	380187.280594	44.224692
3503.933934	380173.433501	44.229697
3503.597186	380166.873219	44.234701
3503.565730	380169.471762	44.239706
3503.721524	380172.778294	44.244711
3503.789859	380174.903254	44.249716
3503.620269	380177.421893	44.254721
3503.535869	380185.191885	44.259725
3503.721811	380177.506204	44.264730
3503.723806	380192.485769	44.269735
3503.679361	380176.926558	44.274740
3503.844608	380156.450887	44.279745
3503.776344	380148.601906	44.284749
3503.744244	380150.284931	44.289754
3503.781980	380145.166060	44.294759
3503.525329	380146.528500	44.299764
3503.833473	380141.621230	44.304769
3503.802375	380151.875330	44.309773
3503.821205	380148.285483	44.314778
3503.930593	380145.596944	44.319783
3503.629882	380134.885231	44.324788
3503.836518	380121.702538	44.329793
3503.790193	380130.433013	44.334797
3503.459591	380123.388508	44.339802
3503.830057	380128.110849	44.344807
3503.755293	380124.434057	44.349812
3504.059892	380125.529754	44.354817
3503.754993	380125.577256	44.359821
3503.847440	380108.826421	44.364826
3504.014541	380093.742420	44.369831
3503.632383	380099.855415	44.374836
3504.015215	380087.102674	44.379841
3503.856954	380094.528283	44.384845
3503.949544	380094.589263	44.389850
3503.639231	380095.273469	44.394855
3503.696726	380094.271770	44.399860
3504.003015	380075.147198	44.404865
3503.380383	380069.751179	44.409869
3503.655720	380059.685986	44.414874
3503.882578	380069.466959	44.419879
3503.622070	380069.736351	44.424884
3503.904042	380070.428683	44.429889
3503.622421	380076.830999	44.434893
3503.667342	380070.286680	44.439898
3503.610022	380079.909094	44.444903
3503.630238	380075.479700	44.449908
3503.579890	380070.756250	44.454913
3503.401326	380079.304166	44.459917
3503.574484	380073.960410	44.464922
3503.810300	380074.583735	44.469927
3503.684955	380054.840656	44.474932
3503.420966	380049.031874	44.479937
3503.504693	380049.908143	44.484941
3503.456624	380045.514972	44.489946
3503.558465	380049.847401	44.494951
3503.505010	380052.983542	44.499956
3503.779913	380049.251478	44.504961
3503.195999	380064.654337	44.509965
3503.633529	380054.792414	44.514970
3503.930853	380052.404807	44.519975
3503.539363	380060.045322	44.524980
3503.678844	380050.230505	44.529985
3503.775438	380058.099087	44.534989
3504.061349	380050.931694	44.539994
3503.641592	380066.715551	44.544999
3503.526118	380053.456575	44.550004
3503.892897	380037.908616	44.555009
3504.075997	380029.485769	44.560013
3504.229255	380024.653832	44.565018
3504.555209	380027.450236	44.570023
3504.291066	380006.737143	44.575028
3503.986991	379992.922972	44.580033
3503.980954	380003.045980	44.585037
3504.093365	379992.625010	44.590042
3503.794879	379982.955698	44.595047
3503.974279	379975.092973	44.600052
3503.963753	379952.915460	44.605057
3503.947795	379971.763924	44.610061
3503.696716	379974.142851	44.615066
3504.171690	379977.551557	44.620071
3503.933259	379959.504949	44.625076
3504.036677	379946.313076	44.630081
3503.866959	379941.455873	44.635085
3503.781977	379936.865051	44.640090
3503.940495	379935.415002	44.645095
3503.640179	379937.979752	44.650100
3504.150954	379925.613681	44.655105
3503.982772	379907.708550	44.660109
3503.983326	379902.798997	44.665114
3503.796619	379899.089007	44.670119
3503.708342	379903.273462	44.675124
3504.179664	379901.494198	44.680129
3503.637168	379881.257411	44.685133
3504.015200	379869.471853	44.690138
3503.648382	379862.433024	44.695143
3503.395333	379862.752106	44.700148
3504.033905	379859.191453	44.705153
3503.857096	379866.340261	44.710157
3503.965541	379865.712015	44.715162
3504.087102	379866.022758	44.720167
3504.073766	379849.364832	44.725172
3503.910509	379835.350310	44.730177
3503.991831	379843.653729	44.735181
3503.906893	379830.796797	44.740186
3503.977691	379836.126087	44.745191
3504.012845	379812.847607	44.750196
3503.859293	379799.263918	44.755201
3503.946679	379804.056474	44.760205
3503.839445	379803.538618	44.765210
3504.072952	379809.554352	44.770215
3504.050290	379789.998381	44.775220
3503.969690	379772.460858	44.780225
3503.671063	379767.420534	44.785229
3504.043221	379773.363491	44.790234
3503.813299	379770.804857	44.795239
3503.921772	379786.530775	44.800244
3504.212172	379749.858979	44.805249
3504.202719	379744.976421	44.810253
3504.245757	379732.455308	44.815258
3503.699139	379732.337539	44.820263
3503.702156	379736.939964	44.825268
3503.875583	379712.901979	44.830273
3503.630517	379711.846353	44.835277
3503.723247	379710.432128	44.840282
3503.584354	379708.062576	44.845287
3503.611169	379708.769808	44.850292
3503.933006	379708.972597	44.855297
3503.917698	379706.023959	44.860301
3503.825712	379703.214612	44.865306
3504.060946	379700.938535	44.870311
3503.921540	379682.316594	44.875316
3504.151587	379678.438978	44.880321
3503.607648	379681.830710	44.885325
3503.871804	379664.111478	44.890330
3503.811477	379666.307670	44.895335
3503.781639	379671.500283	44.900340
3503.954305	379637.263241	44.905345
3503.646392	379634.309976	44.910349
3503.782257	379634.389552	44.915354
3503.694118	379634.580834	44.920359
3503.853876	379628.730451	44.925364
3503.883666	379627.453341	44.930369
3503.469236	379643.363699	44.935373
3503.745483	379631.288945	44.940378
3504.018810	379635.619751	44.945383
3503.752930	379616.280175	44.950388
3504.029913	379597.414343	44.955393
3503.401045	379599.573225	44.960397
3503.599213	379597.328434	44.965402
3503.544805	379601.278659	44.970407
3503.604710	379601.039595	44.975412
3503.928830	379600.936812	44.980417
3503.780217	379606.987537	44.985421
3503.819353	379607.947166	44.990426
3503.798432	379598.996918	44.995431
3503.647459	379585.921433	45.000436
3503.604418	379581.476546	45.005441
3503.766606	379582.035213	45.010445
3503.774563	379569.061775	45.015450
3503.957059	379579.841822	45.020455
3503.817507	379579.100161	45.025460
3504.181178	379572.047563	45.030465
3503.687518	379564.214829	45.035469
3503.964360	379543.670329	45.040474
3504.076404	379539.480704	45.045479
3503.833909	379540.205070	45.050484
3504.220699	379537.854161	45.055489
3503.574591	379547.213683	45.060493
3504.062577	379524.601057	45.065498
3503.755477	379519.155090	45.070503
3503.708213	379519.848599	45.075508
3503.790864	379504.065557	45.080513
3503.758162	379512.336199	45.085517
3503.538619	379514.862776	45.090522
3503.917468	379518.235847	45.095527
3503.663807	379523.896238	45.100532
3503.534182	379522.618887	45.105537
3503.939261	379515.890380	45.110541
3503.854760	379496.064258	45.115546
3503.431668	379497.351289	45.120551
3503.758873	379496.357816	45.125556
3503.973371	379482.614109	45.130561
3503.393532	379489.317998	45.135565
3503.746046	379485.293836	45.140570
3503.821827	379480.550380	45.145575
3503.831134	379492.019116	45.150580
3503.690800	379491.201275	45.155585
3503.489485	379500.795721	45.160589
3503.871263	379492.163317	45.165594
3503.482004	379481.287378	45.170599
3503.624694	379478.593530	45.175604
3504.038122	379470.566543	45.180609
3503.836602	379474.794377	45.185613
3503.955340	379473.706679	45.190618
3504.030161	379474.202853	45.195623
3503.993474	379480.312211	45.200628
3503.958635	379449.566874	45.205633
3503.996606	379447.245656	45.210637
3503.735605	379443.216718	45.215642
3503.667141	379441.344706	45.220647
3503.501818	379439.920388	45.225652
3504.031836	379428.670233	45.230657
3503.850455	379434.548123	45.235661
3503.407866	379423.121039	45.240666
3503.377259	379407.406727	45.245671
3503.444627	379403.427624	45.250676
3503.322824	379406.065931	45.255681
3503.501010	379434.727086	45.260685
3503.683394	379429.280047	45.265690
3503.872700	379424.696682	45.270695
3503.884004	379418.004961	45.275700
3503.938429	379405.888893	45.280705
3503.850258	379418.110656	45.285709
3503.770730	379414.714328	45.290714
3504.086009	379411.611682	45.295719
3504.144614	379393.161782	45.300724
3504.012360	379373.165104	45.305729
3503.683602	379372.783991	45.310733
3503.720550	379368.860561	45.315738
3503.775362	379374.446786	45.320743
3503.708450	379375.270575	45.325748
3504.069474	379370.965278	45.330753
3503.561296	379359.904624	45.335757
3503.355496	379342.869950	45.340762
3503.782923	379350.838993	45.345767
3503.803664	379338.677360	45.350772
3503.793301	379338.958089	45.355777
3503.677601	379361.358001	45.360781
3503.635173	379348.417887	45.365786
3503.794339	379347.247493	45.370791
3503.584924	379348.933143	45.375796
3504.011728	379355.325348	45.380801
3503.702537	379342.325656	45.385805
3503.875204	379326.375708	45.390810
3503.941342	379316.063609	45.395815
3503.661738	379315.623857	45.400820
3503.627842	379313.720942	45.405825
3503.672531	379313.204502	45.410829
3503.816604	379310.306948	45.415834
3503.777678	379314.763445	45.420839
3503.805856	379322.236037	45.425844
3504.048910	379305.588225	45.430849
3503.731072	379287.401249	45.435853
3503.673754	379284.408350	45.440858
3503.757535	379284.572462	45.445863
3503.929276	379285.790921	45.450868
3503.937690	379274.648596	45.455873
3504.108256	379283.955409	45.460877
3504.023267	379271.174603	45.465882
3503.706262	379252.987479	45.470887
3503.618700	379251.042173	45.475892
3504.095801	379246.184391	45.480897
3503.757462	379253.384276	45.485901
3503.575129	379244.306850	45.490906
3503.794479	379254.114651	45.495911
3503.766582	379254.474455	45.500916
3503.818719	379228.166236	45.505921
3503.836672	379226.534901	45.510925
3503.604521	379223.569630	45.515930
3504.112966	379217.257123	45.520935
3504.176067	379226.682673	45.525940
3504.138023	379215.929191	45.530945
3504.295594	379195.734009	45.535949
3503.908966	379184.654094	45.540954
3504.005852	379187.664806	45.545959
3503.816539	379185.379494	45.550964
3504.090113	379166.005303	45.555969
3503.703632	379158.486196	45.560973
3503.691578	379148.084673	45.565978
3503.675551	379145.593929	45.570983
3503.223269	379153.269663	45.575988
3503.655925	379145.748263	45.580993
3503.618084	379149.823089	45.585997
3503.893454	379146.014561	45.591002
3503.841806	379144.521396	45.596007
3503.399041	379147.235884	45.601012
3503.823218	379143.734487	45.606017
3503.780643	379148.674837	45.611021
3503.870875	379128.973519	45.616026
3503.764590	379116.297767	45.621031
3503.769300	379112.659187	45.626036
3503.999646	379108.959511	45.631041
3503.839067	379116.741756	45.636045
3503.933349	379114.869441	45.641050
3503.712483	379115.615830	45.646055
3503.687474	379108.446537	45.651060
3503.845902	379083.800106	45.656065
3503.649481	379090.392594	45.661069
3503.908406	379082.491686	45.666074
3504.085870	379069.364118	45.671079
3503.822693	379082.503857	45.676084
3503.860934	379073.467834	45.681089
3503.993173	379075.887970	45.686093
3503.989334	379042.950036	45.691098
3504.063655	379037.265675	45.696103
3503.828613	379036.157577	45.701108
3503.974411	379040.737517	45.706113
3503.720723	379042.023223	45.711117
3503.797409	379023.926376	45.716122
3503.920242	379007.806132	45.721127
3503.723140	379007.862031	45.726132
3503.627332	378997.600878	45.731137
3503.668718	379010.285551	45.736141
3503.695611	379008.983445	45.741146
3503.469112	379007.543344	45.746151
3503.624058	379010.875544	45.751156
3503.926399	379004.671881	45.756161
3503.727762	379017.776007	45.761165
3503.930177	379012.249440	45.766170
3504.097901	378986.762134	45.771175
3504.087260	378976.741862	45.776180
3504.110472	378966.512759	45.781185
3504.007121	378974.616638	45.786189
3504.035499	378966.650406	45.791194
3503.851032	378945.669809	45.796199
3503.642777	378954.426140	45.801204
3503.946255	378938.302752	45.806209
3503.770968	378956.388411	45.811213
3503.667477	378956.505819	45.816218
3503.739984	378959.876487	45.821223
3503.506801	378962.888514	45.826228
3503.792131	378961.647299	45.831233
3503.707511	378936.327017	45.836237
3503.900699	378925.231693	45.841242
3503.819251	378916.545202	45.846247
3503.337564	378920.842809	45.851252
3503.824565	378914.228426	45.856257
3503.654661	378919.112625	45.861261
3503.641209	378924.073835	45.866266
3503.997310	378915.877753	45.871271
3503.647083	378922.799795	45.876276
3503.961275	378911.252952	45.881281
3503.515429	378904.760569	45.886285
3503.756072	378890.503827	45.891290
3504.130160	378881.541853	45.896295
3503.518633	378885.173247	45.901300
3503.613016	378876.840479	45.906305
3503.689272	378889.036419	45.911309
3503.459125	378888.080151	45.916314
3503.923912	378881.698186	45.921319
3503.891623	378884.296946	45.926324
3503.554255	378884.349579	45.931329
3503.665466	378886.467834	45.936333
3503.804855	378869.225787	45.941338
3503.931789	378855.088744	45.946343
3503.490957	378860.549900	45.951348
3503.974881	378847.246648	45.956353
3503.809814	378853.630742	45.961357
3503.742099	378855.039669	45.966362
3503.830416	378850.853721	45.971367
3504.008392	378850.824904	45.976372
3504.100061	378833.361471	45.981377
3503.911279	378828.379968	45.986381
3504.066673	378816.527543	45.991386
3504.115148	378820.995717	45.996391
3503.868054	378812.920384	46.001396
3503.954455	378784.520798	46.006401
3504.145621	378780.903588	46.011405
3504.023258	378773.037446	46.016410
3503.865029	378780.412429	46.021415
3504.047434	378774.303990	46.026420
3504.138290	378741.045618	46.031425
3503.878744	378741.747258	46.036429
3503.665889	378729.724095	46.041434
3503.858138	378735.186949	46.046439
3504.104771	378746.542091	46.051444
3504.148817	378729.340487	46.056449
3503.794813	378717.390499	46.061453
3503.729201	378705.522101	46.066458
3503.514740	378707.284879	46.071463
3503.685629	378709.164797	46.076468
3503.795201	378712.504193	46.081473
3503.747064	378711.366545	46.086477
3503.874051	378705.979031	46.091482
3504.005763	378692.171827	46.096487
3503.728728	378684.686201	46.101492
3503.875723	378671.054619	46.106497
3503.800197	378669.794123	46.111501
3503.834542	378669.813442	46.116506
3503.657397	378677.471218	46.121511
3503.680848	378681.383796	46.126516
3503.724883	378675.551560	46.131521
3503.691918	378686.111558	46.136525
3503.435391	378661.428706	46.141530
3503.681615	378658.896483	46.146535
3503.464559	378638.734789	46.151540
3503.722148	378631.597049	46.156545
3503.565191	378643.982534	46.161549
3503.878614	378636.123793	46.166554
3503.512220	378639.792771	46.171559
3503.524902	378642.994877	46.176564
3503.923918	378642.931125	46.181569
3503.521246	378642.917775	46.186573
3503.468580	378648.012392	46.191578
3503.715401	378648.990090	46.196583
3503.688719	378646.246650	46.201588
3503.667178	378641.391300	46.206593
3503.573261	378644.661124	46.211597
3503.841033	378647.950088	46.216602
3504.217198	378627.643760	46.221607
3503.546873	378619.457233	46.226612
3503.724558	378611.670811	46.231617
3503.566704	378611.542462	46.236621
3503.499050	378607.813533	46.241626
3503.759924	378605.787690	46.246631
3503.471638	378609.673240	46.251636
3503.667278	378616.305582	46.256641
3503.661121	378614.627162	46.261645
3503.852563	378609.331188	46.266650
3503.971478	378609.235400	46.271655
3503.881030	378583.915812	46.276660
3503.805418	378567.648708	46.281665
3503.840145	378574.026704	46.286669
3503.950329	378575.178610	46.291674
3503.944004	378573.754565	46.296679
3503.924086	378579.683368	46.301684
3504.005991	378551.157150	46.306689
3503.670912	378546.478517	46.311693
3503.622099	378538.168309	46.316698
3503.692339	378551.280964	46.321703
3503.573956	378549.365930	46.326708
3503.768725	378544.705295	46.331713
3503.620736	378549.179116	46.336717
3503.839866	378544.183976	46.341722
3504.103648	378546.583355	46.346727
3503.736951	378532.422474	46.351732
3504.026657	378501.218139	46.356737
3503.776136	378514.101717	46.361741
3503.941285	378508.911625	46.366746
3503.723071	378511.946755	46.371751
3503.526266	378524.796405	46.376756
3503.817624	378511.269126	46.381761
3503.462486	378518.064839	46.386765
3503.408793	378522.193105	46.391770
3503.720134	378517.488608	46.396775
3503.577961	378511.889258	46.401780
3503.433259	378490.571478	46.406785
3503.417431	378482.103435	46.411789
3503.445113	378479.605741	46.416794
3503.698337	378479.081766	46.421799
3503.617072	378489.039010	46.426804
3503.902837	378478.310454	46.431809
3503.722659	378489.300732	46.436813
3503.960465	378485.650688	46.441818
3504.101927	378482.295656	46.446823
3503.686514	378482.665845	46.451828
3503.867007	378485.129261	46.456833
3503.636360	378474.838413	46.461837
3503.606596	378457.215960	46.466842
3503.544933	378460.175481	46.471847
3503.392204	378466.786603	46.476852
3503.842517	378455.218113	46.481857
3503.562083	378457.296550	46.486861
3503.265023	378458.080428	46.491866
3503.586753	378459.707603	46.496871
3503.469266	378461.480501	46.501876
3503.829188	378451.910228	46.506881
3503.871870	378465.154442	46.511885
3503.972357	378458.295851	46.516890
3504.039376	378460.522853	46.521895
3503.915995	378456.090537	46.526900
3503.925773	378442.251647	46.531905
3503.553988	378438.952295	46.536909
3503.613750	378434.516465	46.541914
3503.421422	378435.538141	46.546919
3503.773127	378439.678648	46.551924
3503.512359	378438.447423	46.556929
3503.411980	378442.048940	46.561933
3503.382475	378437.907005	46.566938
3503.589701	378435.813327	46.571943
3503.486923	378448.724446	46.576948
3503.741347	378438.814753	46.581953
3503.871566	378439.251315	46.586957
3503.675767	378438.594828	46.591962
3503.630519	378448.215734	46.596967
3503.578875	378442.932722	46.601972
3504.108432	378427.968840	46.606977
3503.641097	378416.825158	46.611981
3503.515958	378408.120025	46.616986
3503.648426	378408.301881	46.621991
3503.398062	378407.704887	46.626996
3503.868482	378406.663317	46.632001
3503.984611	378410.790190	46.637005
3503.461964	378411.558853	46.642010
3503.682984	378411.268882	46.647015
3503.675629	378409.514338	46.652020
3504.075892	378403.778371	46.657025
3503.352798	378392.929456	46.662029
3503.793762	378379.760012	46.667034
3504.153168	378367.188461	46.672039
3503.746630	378370.507718	46.677044
3503.799298	378369.252387	46.682049
3503.935815	378368.975772	46.687053
3503.799140	378365.766430	46.692058
3503.634056	378381.637888	46.697063
3503.668731	378376.112309	46.702068
3503.972764	378349.687384	46.707073
3503.983226	378338.595340	46.712077
3503.665849	378333.583228	46.717082
3503.797843	378335.113220	46.722087
3503.692676	378340.292480	46.727092
3503.810720	378338.365503	46.732097
3503.936239	378339.616732	46.737101
3503.778169	378317.741399	46.742106
3504.028570	378297.531083	46.747111
3503.611993	378306.600270	46.752116
3503.842042	378296.414608	46.757121
3503.733457	378302.357467	46.762125
3503.902722	378299.761079	46.767130
3503.639565	378293.951903	46.772135
3503.611863	378307.258165	46.777140
3503.837839	378301.982127	46.782145
3503.596891	378278.288541	46.787149
3503.504077	378268.535427	46.792154
3503.663180	378269.984832	46.797159
3503.542336	378270.537382	46.802164
3503.716042	378268.779650	46.807169
3503.887772	378263.079782	46.812173
3503.653000	378267.236694	46.817178
3504.107986	378266.248431	46.822183
3504.074727	378269.686745	46.827188
3504.060704	378244.609211	46.832193
3503.565599	378238.963863	46.837197
3503.903243	378235.399757	46.842202
3503.887905	378228.712044	46.847207
3503.686905	378235.305398	46.852212
3503.873983	378224.007361	46.857217
3503.506212	378229.762279	46.862221
3503.515957	378231.108115	46.867226
3503.957807	378229.842140	46.872231
3503.385316	378216.578467	46.877236
3503.581986	378205.253474	46.882241
3503.632503	378201.582135	46.887245
3503.856625	378197.222042	46.892250
3503.769584	378194.488110	46.897255
3503.445837	378203.542648	46.902260
3503.809173	378193.844598	46.907265
3503.787180	378201.655990	46.912269
3503.797701	378194.887879	46.917274
3504.114149	378197.584177	46.922279
3503.947812	378183.188022	46.927284
3503.854934	378176.054721	46.932289
3503.560817	378174.269184	46.937293
3503.622705	378164.720511	46.942298
3503.793832	378168.762410	46.947303
3503.596189	378173.422168	46.952308
3503.773126	378165.508600	46.957313
3503.822085	378160.413132	46.962317
3503.742215	378177.085131	46.967322
3503.875185	378164.523869	46.972327
3503.700403	378147.788996	46.977332
3503.464087	378132.844307	46.982337
3503.310627	378126.687111	46.987341
3503.530086	378125.608894	46.992346
3504.182547	378122.452856	46.997351
3503.269186	378132.490832	47.002356
3503.815839	378127.571051	47.007361
3503.816198	378124.848736	47.012365
3503.759852	378136.150199	47.017370
3503.754225	378134.929509	47.022375
3503.714725	378140.886909	47.027380
3503.753725	378126.916114	47.032385
3503.395511	378114.407032	47.037389
3503.234320	378112.397001	47.042394
3503.686909	378126.390471	47.047399
3503.497685	378132.168053	47.052404
3503.450075	378110.682111	47.057409
3503.444481	378118.872457	47.062413
3503.826523	378126.238478	47.067418
3504.105879	378103.149305	47.072423
3503.777198	378103.912752	47.077428
3503.772102	378099.995841	47.082433
3503.872661	378104.379559	47.087437
3503.984353	378103.877949	47.092442
3503.856553	378106.771643	47.097447
3503.411533	378085.780897	47.102452
3503.684792	378066.253603	47.107457
3503.808957	378071.447523	47.112461
3503.562812	378072.655761	47.117466
3503.529094	378068.590758	47.122471
3503.409326	378064.361309	47.127476
3503.571070	378066.853150	47.132481
3503.716056	378073.925989	47.137485
3503.731236	378073.973772	47.142490
3503.778089	378076.483771	47.147495
3503.539375	378067.694773	47.152500
3503.771610	378068.700226	47.157505
3503.927544	378071.167550	47.162509
3503.855053	378065.938653	47.167514
3503.993933	378047.577176	47.172519
3503.755693	378046.266072	47.177524
3503.994072	378032.289167	47.182529
3503.412805	378046.827596	47.187533
3503.493522	378037.759186	47.192538
3503.790471	378043.510813	47.197543
3503.282436	378051.780583	47.202548
3503.797340	378033.792069	47.207553
3503.776005	378039.975531	47.212557
3503.869903	378047.514284	47.217562
3503.679251	378015.724169	47.222567
3503.714930	378012.462122	47.227572
3503.777726	377995.231800	47.232577
3503.829698	378002.599141	47.237581
3503.885283	378007.015413	47.242586
3504.049456	378000.782561	47.247591
3503.365652	378009.232732	47.252596
3503.665205	378001.579540	47.257601
3503.696122	378007.424089	47.262605
3503.476153	377996.088580	47.267610
3503.561949	377993.200141	47.272615
3503.473124	377975.510502	47.277620
3503.614926	377967.856801	47.282625
3503.338549	377980.185062	47.287629
3503.314227	377984.588531	47.292634
3503.731922	377985.234016	47.297639
3503.510204	377977.179935	47.302644
3503.648449	377962.303160	47.307649
3503.947773	377975.176317	47.312653
3503.514111	377975.447652	47.317658
3503.716759	377970.200692	47.322663
3503.754376	377974.721549	47.327668
3503.930961	377970.496121	47.332673
3503.376740	377968.649942	47.337677
3503.622723	377970.899557	47.342682
3503.952639	377970.846727	47.347687
3503.605416	377976.369515	47.352692
3503.528610	377974.524187	47.357697
3503.588036	377973.751047	47.362701
3503.605856	377962.861217	47.367706
3503.188251	377943.850019	47.372711
3503.399342	377953.557709	47.377716
3503.436153	377968.761539	47.382721
3503.304759	377986.560917	47.387725
3503.407040	377989.596303	47.392730
3504.054805	377986.619044	47.397735
3503.221320	377974.642871	47.402740
3503.594648	377961.789202	47.407745
3503.627517	377954.585117	47.412749
3503.867587	377944.982793	47.417754
3503.989761	377936.798046	47.422759
3503.686664	377954.293917	47.427764
3503.630011	377945.247197	47.432769
3503.948201	377949.087829	47.437773
3503.748980	377952.984802	47.442778
3503.946045	377951.782942	47.447783
3503.557627	377935.844804	47.452788
3503.370019	377932.236511	47.457793
3503.388234	377928.315899	47.462797
3503.835167	377926.286050	47.467802
3503.844409	377925.241052	47.472807
3503.928572	377928.609966	47.477812
3503.931174	377926.904697	47.482817
3503.943135	377924.892725	47.487821
3503.882043	377923.833407	47.492826
3503.918213	377912.889793	47.497831
3503.708038	377894.914073	47.502836
3503.967612	377887.292614	47.507841
3503.609271	377888.849250	47.512845
3503.877153	377884.405901	47.517850
3503.658958	377886.779755	47.522855
3503.563049	377891.804998	47.527860
3503.536026	377884.534059	47.532865
3503.725957	377884.681400	47.537869
3503.474026	377890.240010	47.542874
3503.656828	377884.792692	47.547879
3503.657088	377894.203058	47.552884
3503.396626	377882.416079	47.557889
3503.334773	377880.619254	47.562893
3503.098313	377882.919689	47.567898
3503.400596	377887.525903	47.572903
3503.533699	377887.377001	47.577908
3503.669466	377893.281302	47.582913
3504.015994	377894.548486	47.587917
3503.816700	377884.049044	47.592922
3503.952413	377857.243428	47.597927
3503.608153	377862.689457	47.602932
3503.581481	377861.192296	47.607937
3503.427204	377864.471724	47.612941
3503.444423	377857.015740	47.617946
3503.944465	377856.503619	47.622951
3503.619834	377862.480690	47.627956
3503.728261	377849.897771	47.632961
3503.627587	377864.665534	47.637965
3503.765648	377850.068535	47.642970
3504.109748	377853.752468	47.647975
3503.808992	377835.536684	47.652980
3504.104565	377821.932197	47.657985
3503.829989	377815.132773	47.662989
3503.847603	377817.800023	47.667994
3503.903175	377818.451873	47.672999
3503.571344	377819.571920	47.678004
3503.742789	377792.862354	47.683009
3503.614146	377791.355871	47.688013
3503.414672	377783.654332	47.693018
3503.695906	377794.927972	47.698023
3503.495077	377794.323139	47.703028
3503.565207	377784.900249	47.708033
3503.692048	377794.239762	47.713037
3503.625652	377791.756894	47.718042
3504.007264	377792.840488	47.723047
3503.801551	377790.176155	47.728052
3503.923937	377794.912554	47.733057
3503.775087	377786.185596	47.738061
3503.783786	377777.764396	47.743066
3503.702673	377753.434783	47.748071
3503.513590	377757.737140	47.753076
3503.660582	377751.049125	47.758081
3503.721506	377765.664206	47.763085
3503.738731	377763.244427	47.768090
3503.522180	377754.299242	47.773095
3503.475388	377756.798627	47.778100
3503.623799	377761.836142	47.783105
3503.609413	377760.642261	47.788109
3503.361865	377762.715536	47.793114
3503.599459	377758.124347	47.798119
3503.620432	377767.684082	47.803124
3503.903507	377755.989208	47.808129
3503.873557	377763.242364	47.813133
3503.690808	377751.010660	47.818138
3504.128474	377720.138422	47.823143
3503.726106	377727.857413	47.828148
3503.359360	377722.598670	47.833153
3503.456418	377727.873226	47.838157
3503.472934	377727.157734	47.843162
3503.334684	377728.857639	47.848167
3503.318496	377725.349412	47.853172
3503.680201	377721.908636	47.858177
3503.479317	377731.478008	47.863181
3503.571749	377733.039712	47.868186
3503.792563	377724.864767	47.873191
3503.420601	377729.399515	47.878196
3503.369802	377731.034727	47.883201
3503.791996	377737.478798	47.888205
3503.730194	377729.297650	47.893210
3504.021467	377731.667298	47.898215
3503.738571	377733.059403	47.903220
3504.111213	377714.940617	47.908225
3503.444786	377709.042479	47.913229
3503.573751	377701.289013	47.918234
3504.007201	377692.571744	47.923239
3503.442752	377697.391273	47.928244
3503.836752	377695.471522	47.933249
3503.815270	377694.940083	47.938253
3503.836980	377694.554432	47.943258
3503.931394	377689.960429	47.948263
3503.944212	377677.189083	47.953268
3504.134705	377656.937039	47.958273
3503.696944	377663.415294	47.963277
3503.687538	377655.938045	47.968282
3503.991015	377655.584167	47.973287
3503.863100	377658.020072	47.978292
3503.736823	377647.254672	47.983297
3503.419240	377621.741446	47.988301
3503.647309	377611.403308	47.993306
3503.553486	377609.484346	47.998311
3503.588505	377617.312279	48.003316
3503.899046	377613.192819	48.008321
3503.829748	377617.628873	48.013325
3503.750745	377624.788064	48.018330
3503.946047	377614.277057	48.023335
3504.078935	377613.822962	48.028340
3503.621578	377604.585140	48.033345
3503.792350	377588.354999	48.038349
3503.961714	377579.933800	48.043354
3504.178413	377575.473070	48.048359
3503.737048	377592.456805	48.053364
3503.841343	377577.305460	48.058369
3504.075450	377580.523527	48.063373
3503.847429	377552.376236	48.068378
3503.956107	377548.873693	48.073383
3503.761635	377539.899535	48.078388
3503.439626	377541.272393	48.083393
3503.509698	377539.505573	48.088397
3503.674290	377538.944724	48.093402
3503.670371	377545.227252	48.098407
3503.438882	377542.516105	48.103412
3503.529569	377546.723396	48.108417
3503.590938	377549.943331	48.113421
3503.454652	377548.666967	48.118426
3503.809200	377544.718595	48.123431
3503.410704	377544.679147	48.128436
3503.963762	377538.257581	48.133441
3503.644900	377530.447683	48.138445
3503.471303	377513.178206	48.143450
3503.724459	377500.775788	48.148455
3503.313393	377519.153726	48.153460
3503.834166	377506.149429	48.158465
3503.683859	377514.133851	48.163469
3503.619394	377511.879581	48.168474
3503.667017	377510.701327	48.173479
3503.324043	377518.614456	48.178484
3503.683080	377531.198528	48.183489
3503.761374	377523.910878	48.188493
3503.825501	377512.860992	48.193498
3503.719021	377517.506418	48.198503
3503.783450	377533.748911	48.203508
3503.888871	377516.893179	48.208513
3503.693745	377493.141010	48.213517
3503.616584	377486.157715	48.218522
3503.632094	377483.814496	48.223527
3503.423332	377484.508130	48.228532
3503.426881	377476.952493	48.233537
3503.430088	377489.465638	48.238541
3503.496293	377482.205327	48.243546
3503.702869	377480.467801	48.248551
3503.707249	377485.528116	48.253556
3503.647349	377485.816688	48.258561
3503.980355	377484.237229	48.263565
3503.637496	377483.146126	48.268570
3503.622490	377479.739433	48.273575
3503.842980	377485.299740	48.278580
3503.841870	377474.082105	48.283585
3503.317039	377468.695700	48.288589
3503.597827	377457.942219	48.293594
3503.840645	377442.285652	48.298599
3503.745018	377450.668415	48.303604
3503.140290	377446.515546	48.308609
3503.661011	377446.203638	48.313613
3503.368950	377452.023008	48.318618
3503.638338	377455.388123	48.323623
3503.802422	377447.400137	48.328628
3503.787205	377443.052354	48.333633
3503.571797	377456.337697	48.338637
3503.491647	377457.036440	48.343642
3503.813961	377455.891077	48.348647
3503.542019	377457.713866	48.353652
3503.488692	377455.610447	48.358657
3503.758897	377459.000868	48.363661
3503.394445	377460.355001	48.368666
3503.663319	377451.256720	48.373671
3503.718191	377458.013248	48.378676
3503.692973	377434.132447	48.383681
3503.700189	377422.913481	48.388685
3503.645536	377419.665663	48.393690
3503.957659	377412.519086	48.398695
3503.728149	377422.576335	48.403700
3503.828741	377411.775015	48.408705
3503.928033	377407.358259	48.413709
3503.560602	377417.640793	48.418714
3503.734516	377423.768056	48.423719
3503.627813	377414.245848	48.428724
3504.167818	377395.439137	48.433729
3503.856756	377395.360434	48.438733
3503.635833	377387.992871	48.443738
3503.912688	377390.135898	48.448743
3503.509250	377392.539059	48.453748
3503.805583	377395.442078	48.458753
3503.589025	377402.902843	48.463757
3503.734678	377394.459916	48.468762
3503.846641	377380.935170	48.473767
3503.698194	377368.443570	48.478772
3504.083055	377357.037721	48.483777
3503.532721	377365.695853	48.488781
3503.665650	377360.765061	48.493786
3503.834763	377355.879420	48.498791
3503.677193	377370.452873	48.503796
3503.895499	377370.493989	48.508801
3503.822862	377370.530217	48.513805
3503.741087	377348.464241	48.518810
3503.760454	377325.771808	48.523815
3503.458298	377329.227267	48.528820
3503.808306	377318.284758	48.533825
3503.751069	377327.780653	48.538829
3503.476880	377320.396061	48.543834
3503.815632	377321.461006	48.548839
3503.802224	377324.463857	48.553844
3503.505447	377321.661270	48.558849
3503.506409	377324.331185	48.563853
3503.799786	377319.731129	48.568858
3503.960108	377323.749387	48.573863
3503.629590	377312.787255	48.578868
3503.624804	377285.698231	48.583873
3503.528553	377289.350071	48.588877
3503.598657	377293.840436	48.593882
3503.925615	377286.920413	48.598887
3503.724032	377293.132479	48.603892
3503.648634	377283.478113	48.608897
3503.664367	377292.148538	48.613901
3503.606099	377286.179653	48.618906
3503.846547	377293.034057	48.623911
3503.739457	377290.404975	48.628916
3503.772506	377271.576586	48.633921
3503.579251	377265.171188	48.638925
3503.779257	377250.055463	48.643930
3503.919330	377245.021784	48.648935
3503.599704	377249.090470	48.653940
3503.861667	377252.355033	48.658945
3503.306306	377257.910816	48.663949
3503.703915	377253.675816	48.668954
3503.666407	377251.569885	48.673959
3503.324362	377256.812160	48.678964
3503.683786	377250.522895	48.683969
3503.594103	377261.880747	48.688973
3503.665404	377257.621013	48.693978
3503.736859	377252.496436	48.698983
3503.799564	377239.818809	48.703988
3503.755737	377220.799060	48.708993
3503.616379	377217.869843	48.713997
3503.666313	377211.298821	48.719002
3503.965953	377212.344516	48.724007
3503.626263	377225.369784	48.729012
3503.610348	377220.818600	48.734017
3503.721925	377226.167235	48.739021
3503.600521	377219.368936	48.744026
3503.973976	377226.507561	48.749031
3503.462875	377219.236701	48.754036
3503.741384	377204.998805	48.759041
3503.391530	377198.109430	48.764045
3503.279124	377187.138227	48.769050
3503.645212	377195.346326	48.774055
3503.372736	377197.347262	48.779060
3503.660592	377185.346236	48.784065
3503.469437	377184.587249	48.789069
3503.424710	377190.265823	48.794074
3503.716166	377186.683489	48.799079
3503.794734	377190.333144	48.804084
3503.742565	377189.628498	48.809089
3503.606949	377193.642671	48.814093
3503.481412	377190.584088	48.819098
3503.814521	377179.389854	48.824103
3503.589069	377190.235032	48.829108
3503.640999	377186.944913	48.834113
3504.143957	377189.586368	48.839117
3503.697935	377183.983982	48.844122
3503.843237	377166.613081	48.849127
3503.739321	377156.022065	48.854132
3503.713845	377148.928799	48.859137
3503.156143	377156.138297	48.864141
3503.164305	377148.530996	48.869146
3503.433708	377149.352549	48.874151
3503.555262	377154.089156	48.879156
3503.509650	377151.017938	48.884161
3503.852895	377152.845254	48.889165
3503.513069	377154.093761	48.894170
3503.497886	377149.695069	48.899175
3503.344413	377161.215647	48.904180
3503.760157	377156.621668	48.909185
3503.702949	377161.030426	48.914189
3503.747131	377155.604917	48.919194
3503.657041	377156.228929	48.924199
3503.672438	377162.254106	48.929204
3503.545879	377148.131082	48.934209
3503.803782	377163.223970	48.939213
3503.583969	377159.849619	48.944218
3503.747149	377155.753403	48.949223
3503.472867	377137.787473	48.954228
3504.132857	377125.753049	48.959233
3503.429677	377120.038682	48.964237
3503.516100	377127.553355	48.969242
3503.828086	377118.092083	48.974247
3503.530686	377122.538806	48.979252
3503.605962	377119.194121	48.984257
3503.756776	377123.112159	48.989261
3503.794059	377124.987834	48.994266
3503.746167	377127.894405	48.999271
3503.525224	377130.014379	49.004276
3503.881709	377116.196538	49.009281
3503.667445	377111.981922	49.014285
3503.784358	377091.588605	49.019290
3504.012044	377090.661675	49.024295
3504.097006	377078.947043	49.029300
3503.568751	377084.422258	49.034305
3503.988236	377081.099475	49.039309
3503.947502	377075.051479	49.044314
3503.779165	377051.701787	49.049319
3503.799249	377041.167450	49.054324
3504.111650	377038.014204	49.059329
3503.764334	377044.936111	49.064333
3503.474616	377045.311880	49.069338
3503.913056	377052.999855	49.074343
3503.742988	377048.040605	49.079348
3503.853140	377042.935322	49.084353
3503.793059	377018.271269	49.089357
3503.706684	377006.329335	49.094362
3503.866558	377000.936393	49.099367
3503.512082	377001.678501	49.104372
3503.707567	377000.349683	49.109377
3503.638339	377007.202209	49.114381
3503.489379	377012.515743	49.119386
3503.996782	377009.051879	49.124391
3503.912000	377019.289842	49.129396
3504.022221	377007.774685	49.134401
3503.615777	376990.134807	49.139405
3503.530929	376982.186072	49.144410
3503.328435	376978.427429	49.149415
3503.415697	376984.670198	49.154420
3503.847927	376970.865771	49.159425
3503.231381	376980.831686	49.164429
3503.125194	376980.618858	49.169434
3503.283077	376970.673186	49.174439
3502.947362	376990.921720	49.179444
3503.299694	377011.773704	49.184449
3503.447315	377021.160985	49.189453
3503.396687	377018.751885	49.194458
3503.576237	377011.295522	49.199463
3503.543048	377017.150348	49.204468
3503.660558	377018.555501	49.209473
3503.452033	377021.411161	49.214477
3503.402949	377019.815766	49.219482
3503.937411	377013.193568	49.224487
3503.495011	377009.040434	49.229492
3503.269787	376999.358807	49.234497
3503.686878	377016.690391	49.239501
3503.472443	377013.366049	49.244506
3503.876078	377000.634462	49.249511
3503.406844	377004.345278	49.254516
3503.548872	376991.934831	49.259521
3503.712254	376987.533334	49.264525
3503.036848	376988.300729	49.269530
3503.621327	376991.031057	49.274535
3503.612739	376989.251209	49.279540
3503.682936	376982.880435	49.284545
3503.592156	376990.855553	49.289549
3503.414044	376989.255114	49.294554
3503.649709	376987.589278	49.299559
3503.531251	376990.201781	49.304564
3503.889211	376993.069654	49.309569
3503.485754	376998.652336	49.314573
3503.587983	377002.400013	49.319578
3503.556738	377002.785803	49.324583
3503.498825	377005.108940	49.329588
3503.702506	376993.884239	49.334593
3503.782819	376998.042355	49.339597
3503.741570	377000.973322	49.344602
3503.815200	376984.987212	49.349607
3503.730844	376978.183017	49.354612
3503.590800	376960.526458	49.359617
3503.597457	376957.090860	49.364621
3503.899834	376960.298188	49.369626
3503.768617	376954.493398	49.374631
3503.718165	376962.538456	49.379636
3503.930946	376958.968537	49.384641
3503.770497	376967.183594	49.389645
3503.847924	376966.254974	49.394650
3503.823304	376939.575825	49.399655
3503.277482	376942.026952	49.404660
3503.612289	376937.089637	49.409665
3503.499217	376932.172236	49.414669
3503.439615	376929.484752	49.419674
3503.565132	376931.371926	49.424679
3503.447926	376936.502399	49.429684
3503.604920	376924.750901	49.434689
3503.723292	376933.049078	49.439693
3503.607786	376928.666218	49.444698
3504.032986	376921.730606	49.449703
3503.706636	376934.092524	49.454708
3503.648422	376930.565433	49.459713
3503.782868	376931.535500	49.464717
3503.594426	376927.927247	49.469722
3503.853788	376935.134828	49.474727
3503.647285	376915.377565	49.479732
3503.763633	376900.885394	49.484737
3503.626923	376897.726811	49.489741
3503.351634	376896.421523	49.494746
3503.748193	376898.825454	49.499751
3503.770193	376906.197735	49.504756
3503.679523	376900.132169	49.509761
3503.868533	376898.524575	49.514765
3504.150878	376904.965448	49.519770
3504.038793	376892.874928	49.524775
3503.790482	376881.594452	49.529780
3503.755379	376872.060799	49.534785
3503.531115	376878.581745	49.539789
3503.512282	376877.820953	49.544794
3503.770371	376868.037472	49.549799
3503.819678	376875.659803	49.554804
3503.442951	376877.321127	49.559809
3503.267226	376874.626557	49.564813
3503.385601	376882.288843	49.569818
3503.636907	376879.628525	49.574823
3503.559661	376879.080453	49.579828
3503.514311	376870.565860	49.584833
3503.784188	376876.347371	49.589837
3503.254354	376884.213850	49.594842
3503.614578	376877.975273	49.599847
3503.974799	376872.372596	49.604852
3503.935084	376853.428331	49.609857
3503.667060	376841.743983	49.614861
3503.632837	376829.615702	49.619866
3503.621493	376826.335554	49.624871
3503.557976	376833.365260	49.629876
3503.997213	376823.451393	49.634881
3503.935405	376825.368179	49.639885
3503.736792	376836.539879	49.644890
3503.724799	376827.307795	49.649895
3503.585818	376834.527480	49.654900
3503.566574	376820.514560	49.659905
3503.605612	376802.702447	49.664909
3503.470252	376799.391026	49.669914
3503.445113	376788.634845	49.674919
3503.442197	376797.181145	49.679924
3503.716482	376797.544084	49.684929
3503.821794	376794.728782	49.689933
3503.629496	376798.853697	49.694938
3503.519482	376798.132751	49.699943
3503.643795	376791.753393	49.704948
3503.467223	376791.602560	49.709953
3503.405136	376795.834076	49.714957
3503.408053	376794.281326	49.719962
3503.673191	376792.738004	49.724967
3503.382488	376799.651006	49.729972
3503.587722	376793.640400	49.734977
3503.641803	376799.074488	49.739981
3503.562395	376801.172110	49.744986
3503.999685	376791.055054	49.749991
3503.701816	376805.040420	49.754996
3503.899436	376806.153122	49.760001
3503.945962	376780.149396	49.765005
3503.709563	376761.541407	49.770010
3503.882074	376753.399334	49.775015
3503.530169	376755.921568	49.780020
3503.739689	376757.922654	49.785025
3503.871307	376755.611914	49.790029
3503.295974	376761.781388	49.795034
3503.751404	376759.495779	49.800039
3503.316549	376760.937370	49.805044
3503.679523	376754.316797	49.810049
3503.542974	376773.618261	49.815053
3503.519024	376773.672231	49.820058
3503.522086	376766.854183	49.825063
3503.250170	376773.052009	49.830068
3503.223469	376764.661627	49.835073
3503.730034	376756.161524	49.840077
3503.462474	376766.479313	49.845082
3503.885464	376764.783861	49.850087
3503.683360	376771.784609	49.855092
3503.718537	376762.977468	49.860097
3503.496987	376742.052437	49.865101
3503.438796	376737.228082	49.870106
3503.772231	376730.586738	49.875111
3503.433474	376737.151240	49.880116
3503.469261	376735.618728	49.885121
3503.714057	376739.038664	49.890125
3503.370059	376735.887393	49.895130
3503.724195	376737.611263	49.900135
3503.436266	376736.536893	49.905140
3503.625525	376725.721374	49.910145
3503.533293	376746.618323	49.915149
3503.438865	376745.615115	49.920154
3503.787039	376732.408922	49.925159
3503.193326	376741.201226	49.930164
3503.562684	376739.412505	49.935169
3503.450732	376739.734745	49.940173
3503.430743	376743.247401	49.945178
3503.990761	376734.484485	49.950183
3503.849195	376736.159519	49.955188
3503.813210	376738.682696	49.960193
3503.542286	376745.897814	49.965197
3503.582212	376742.507812	49.970202
3503.791100	376738.531510	49.975207
3503.522287	376728.042751	49.980212
3503.769763	376710.375707	49.985217
3503.536400	376702.933675	49.990221
3503.484160	376702.966680	49.995226
3503.836045	376702.427091	50.000231
3503.511700	376710.490051	50.005236
3503.529174	376702.016365	50.010241
3503.792477	376698.209513	50.015245
3503.389742	376699.544284	50.020250
3503.667139	376700.237403	50.025255
3503.604308	376700.551879	50.030260
3503.782321	376694.164019	50.035265
3503.820635	376693.216138	50.040269
3503.431948	376701.645376	50.045274
3503.484774	376702.043317	50.050279
3503.362533	376705.343213	50.055284
3503.514705	376704.682571	50.060289
3503.269017	376710.240357	50.065293
3503.316472	376709.316468	50.070298
3503.722594	376704.800268	50.075303
3503.717188	376708.921090	50.080308
3503.627964	376706.340017	50.085313
3503.493760	376710.735557	50.090317
3503.602848	376708.504684	50.095322
3503.729295	376710.875009	50.100327
3503.675481	376691.220683	50.105332
3503.774107	376677.723243	50.110337
3503.476771	376676.395996	50.115341
3503.183031	376672.143022	50.120346
3503.525455	376672.062778	50.125351
3503.213863	376683.506739	50.130356
3503.351332	376679.897826	50.135361
3503.182944	376684.375080	50.140365
3503.435035	376705.751790	50.145370
3503.434939	376716.332552	50.150375
3503.314028	376732.121378	50.155380
3503.412227	376720.531729	50.160385
3503.397566	376724.170726	50.165389
3503.422167	376721.927771	50.170394
3503.916548	376712.971734	50.175399
3503.555996	376719.132705	50.180404
3503.620608	376726.269359	50.185409
3503.752819	376728.104613	50.190413
3503.825184	376708.989949	50.195418
3503.869244	376695.552011	50.200423
3503.482490	376685.285371	50.205428
3503.527691	376676.425755	50.210433
3503.712920	376681.177791	50.215437
3503.317767	376687.420543	50.220442
3503.649092	376673.886324	50.225447
3503.688851	376685.885221	50.230452
3503.365327	376683.875337	50.235457
3503.604055	376697.750496	50.240461
3503.650588	376695.071658	50.245466
3503.659107	376679.985982	50.250471
3503.306229	376692.810018	50.255476
3503.768129	376688.920904	50.260481
3503.989536	376685.527650	50.265485
3503.544085	376684.732536	50.270490
3503.727583	376658.681648	50.275495
3503.720728	376656.799766	50.280500
3503.596325	376656.437198	50.285505
3503.579519	376653.234208	50.290509
3503.607910	376652.186150	50.295514
3503.971630	376646.328527	50.300519
3503.448856	376659.891638	50.305524
3503.831127	376653.674978	50.310529
3504.302025	376655.075164	50.315533
3503.839055	376642.353249	50.320538
3504.050875	376628.888774	50.325543
3503.889746	376624.258729	50.330548
3503.817259	376624.066008	50.335553
3504.148932	376626.403903	50.340557
3503.908065	376617.716667	50.345562
3503.906240	376588.032210	50.350567
3503.645164	376581.586548	50.355572
3503.665650	376573.595647	50.360577
3503.857223	376584.502259	50.365581
3503.438430	376586.831585	50.370586
3503.780830	376576.068131	50.375591
3503.720654	376578.035543	50.380596
3503.746704	376581.795300	50.385601
3503.739009	376581.185359	50.390605
3503.525743	376586.178441	50.395610
3503.904847	376571.517443	50.400615
3503.605847	376557.574082	50.405620
3503.499645	376538.462123	50.410625
3503.691686	376539.830077	50.415629
3503.721056	376545.497031	50.420634
3503.672665	376539.068620	50.425639
3503.839251	376545.578720	50.430644
3503.824583	376529.046786	50.435649
3503.821040	376536.652099	50.440653
3503.643799	376536.882914	50.445658
3503.902383	376528.243903	50.450663
3503.624026	376512.033437	50.455668
3503.661756	376496.205424	50.460673
3503.487448	376502.082629	50.465677
3503.126166	376504.937032	50.470682
3503.176700	376501.240098	50.475687
3502.936899	376517.429342	50.480692
3503.261931	376531.087428	50.485697
3503.460688	376537.414391	50.490701
3503.511532	376550.276409	50.495706
3503.746720	376541.768280	50.500711
3503.566152	376559.652374	50.505716
3503.727272	376554.895081	50.510721
3503.450291	376549.215015	50.515725
3503.456561	376534.384003	50.520730
3503.914007	376510.757037	50.525735
3503.724571	376499.823256	50.530740
3503.600303	376456.371589	50.535745
3503.431891	376419.260498	50.540749
3503.170640	376377.763557	50.545754
3502.899753	376311.136945	50.550759
3502.675880	376261.570638	50.555764
3502.131045	376181.175125	50.560769
3502.001865	376113.635513	50.565773
3501.719250	376033.249134	50.570778
3501.785796	375945.379916	50.575783
3501.626590	375848.287234	50.580788
3501.206885	375741.645835	50.585793
3500.939376	375630.808462	50.590797
3500.600425	375515.963047	50.595802
3500.518991	375380.498094	50.600807
3500.219684	375250.993959	50.605812
3499.472083	375114.590488	50.610817
3499.293580	374984.939228	50.615821
3498.726208	374842.859296	50.620826
3498.589524	374687.686845	50.625831
3497.763000	374538.448025	50.630836
3497.541055	374373.723355	50.635841
3496.965848	374217.041298	50.640845
3496.251290	374062.135877	50.645850
3495.957140	373885.108763	50.650855
3495.659610	373723.293356	50.655860
3495.149430	373543.144605	50.660865
3494.614082	373368.341077	50.665869
3493.912820	373190.790255	50.670874
3493.579971	373007.456794	50.675879
3492.805037	372824.879239	50.680884
3492.297671	372641.749820	50.685889
3491.835279	372455.432642	50.690893
3491.157285	372283.012908	50.695898
3491.238099	372079.564141	50.700903
3490.365227	371889.646107	50.705908
3489.600055	371689.788887	50.710913
3488.963622	371489.732295	50.715917
3488.440400	371290.928838	50.720922
3487.680106	371093.790052	50.725927
3487.096993	370894.307330	50.730932
3486.628048	370685.163924	50.735937
3486.140224	370482.560550	50.740941
3485.390049	370286.510344	50.745946
3484.777218	370069.016871	50.750951
3484.226001	369861.586934	50.755956
3483.831098	369654.411134	50.760961
3483.179303	369437.327672	50.765965
3482.244950	369230.311420	50.770970
3481.689835	369017.459166	50.775975
3481.103310	368804.280100	50.780980
3480.398609	368587.302503	50.785985
3479.837097	368377.221203	50.790989
3478.978503	368170.849402	50.795994
3478.379995	367954.411584	50.800999
3477.511972	367730.815329	50.806004
3477.117842	367525.664600	50.811009
3476.720602	367305.680820	50.816013
3475.976041	367084.198884	50.821018
3475.503046	366864.250325	50.826023
3474.636101	366654.819693	50.831028
3473.871449	366418.403031	50.836033
3473.525676	366205.580405	50.841037
3472.641014	365988.338606	50.846042
3472.208270	365769.217890	50.851047
3471.439370	365551.243281	50.856052
3470.657068	365323.321538	50.861057
3470.106879	365106.251597	50.866061
3469.678684	364885.930046	50.871066
3468.948836	364646.012847	50.876071
3467.614589	364436.035107	50.881076
3467.329221	364211.794864	50.886081
3466.949111	363994.921728	50.891085
3465.751303	363779.372676	50.896090
3465.293520	363541.493070	50.901095
3464.477789	363331.504640	50.906100
3464.223133	363112.444767	50.911105
3463.394679	362890.853793	50.916109
3462.601280	362670.375773	50.921114
3462.023856	362437.267514	50.926119
3461.007875	362218.654548	50.931124
3460.763545	361995.313077	50.936129
3460.418679	361780.561374	50.941133
3459.089757	361555.099204	50.946138
3458.364236	361329.540578	50.951143
3457.880741	361123.739045	50.956148
3457.320331	360903.979258	50.961153
3456.741261	360676.562304	50.966157
3456.002946	360447.719034	50.971162
3455.282906	360228.388491	50.976167
3454.573462	359999.945645	50.981172
3454.042118	359780.303320	50.986177
3453.369409	359556.102037	50.991181
3452.433914	359339.218873	50.996186
3451.879610	359114.666024	51.001191
3451.575353	358898.953424	51.006196
3451.066942	358663.500152	51.011201
3449.971981	358447.452501	51.016205
3449.245374	358223.635287	51.021210
3448.796903	357995.090851	51.026215
3447.529151	357776.751887	51.031220
3446.630272	357554.892833	51.036225
3446.352858	357340.772303	51.041229
3445.523715	357131.776642	51.046234
3445.236245	356919.030039	51.051239
3444.326182	356695.234900	51.056244
3443.617447	356465.197692	51.061249
3443.047717	356255.266681	51.066253
3442.279811	356044.297306	51.071258
3441.913311	355805.067170	51.076263
3440.902476	355589.019234	51.081268
3440.390724	355366.274934	51.086273
3439.623240	355157.846618	51.091277
3438.889991	354939.156302	51.096282
3438.265733	354721.745698	51.101287
3437.891633	354506.661354	51.106292
3437.098603	354285.280133	51.111297
3436.266335	354074.821743	51.116301
3435.161592	353861.835216	51.121306
3435.020656	353637.014311	51.126311
3434.095058	353421.758134	51.131316
3433.457138	353209.331365	51.136321
3433.041077	352988.521245	51.141325
3432.005173	352771.498361	51.146330
3431.423495	352557.074988	51.151335
3430.584351	352349.537424	51.156340
3430.086254	352132.655935	51.161345
3429.314435	351925.233311	51.166349
3428.730493	351711.112261	51.171354
3428.271951	351493.560206	51.176359
3427.378356	351287.884957	51.181364
3426.415909	351068.680212	51.186369
3426.151816	350855.904942	51.191373
3425.424812	350639.867985	51.196378
3424.506002	350430.833966	51.201383
3424.108284	350221.996722	51.206388
3423.527345	350003.999878	51.211393
3422.839743	349786.273532	51.216397
3421.809778	349578.042783	51.221402
3421.625100	349361.558695	51.226407
3420.934208	349150.727604	51.231412
3419.993127	348930.747317	51.236417
3419.090821	348721.984116	51.241421
3418.651507	348508.769268	51.246426
3418.084568	348292.926805	51.251431
3417.371653	348082.095126	51.256436
3416.589965	347867.073968	51.261441
3416.156163	347660.650648	51.266445
3415.159582	347446.043627	51.271450
3414.663107	347234.385531	51.276455
3413.697944	347032.065346	51.281460
3412.825114	346820.312485	51.286465
3412.247209	346615.460719	51.291469
3411.834237	346410.276713	51.296474
3411.190921	346188.584197	51.301479
3410.414030	345988.419467	51.306484
3409.643629	345778.428241	51.311489
3409.138878	345569.895973	51.316493
3408.401020	345354.094804	51.321498
3407.925473	345141.025747	51.326503
3407.545103	344940.667440	51.331508
3406.682438	344735.014058	51.336513
3406.273660	344520.990412	51.341517
3405.270591	344305.634547	51.346522
3404.977847	344074.613496	51.351527
3403.842924	343873.785406	51.356532
3403.170528	343660.309385	51.361537
3402.533392	343444.459821	51.366541
3401.470536	343240.971005	51.371546
3401.052000	343034.834237	51.376551
3400.346832	342828.818438	51.381556
3399.975072	342624.912826	51.386561
3399.058481	342406.532839	51.391565
3398.363328	342200.487858	51.396570
3397.842009	341991.309258	51.401575
3396.947988	341792.319751	51.406580
3396.503308	341580.454905	51.411585
3395.931711	341373.114868	51.416589
3395.024107	341170.154560	51.421594
3394.770211	340958.461048	51.426599
3393.966622	340754.184733	51.431604
3392.828360	340539.676834	51.436609
3392.257294	340333.453250	51.441613
3391.534474	340129.696675	51.446618
3390.801064	339915.529910	51.451623
3390.167772	339719.801712	51.456628
3389.760265	339517.189703	51.461633
3388.966436	339296.921088	51.466637
3388.111334	339105.858962	51.471642
3387.682316	338894.898934	51.476647
3386.755854	338699.188483	51.481652
3386.493843	338494.157376	51.486657
3385.986230	338288.248032	51.491661
3384.988620	338086.946665	51.496666
3384.450230	337872.233088	51.501671
3383.537635	337674.455393	51.506676
3382.829813	337468.855117	51.511681
3382.619390	337265.695730	51.516685
3381.713062	337050.884883	51.521690
3381.236191	336846.315310	51.526695
3380.303582	336645.508356	51.531700
3379.433539	336438.123091	51.536705
3378.782892	336236.659362	51.541709
3377.960093	336038.353425	51.546714
3377.635252	335828.385301	51.551719
3377.045380	335627.470180	51.556724
3376.466560	335413.595089	51.561729
3375.909599	335212.597158	51.566733
3374.902768	335011.542471	51.571738
3374.489299	334803.570835	51.576743
3373.771663	334595.290252	51.581748
3372.906421	334394.567765	51.586753
3372.412152	334194.371561	51.591757
3371.498029	333982.046990	51.596762
3370.961948	333779.692304	51.601767
3370.275040	333594.188413	51.606772
3369.437996	333379.762283	51.611777
3368.905372	333169.666116	51.616781
3368.058466	332976.497612	51.621786
3367.792336	332778.425194	51.626791
3366.689725	332574.552746	51.631796
3366.594998	332370.036653	51.636801
3365.827428	332158.116182	51.641805
3364.850647	331957.022473	51.646810
3364.602998	331750.492123	51.651815
3363.753668	331544.667312	51.656820
3362.947292	331336.136522	51.661825
3362.432005	331135.731312	51.666829
3361.799559	330933.307381	51.671834
3360.963953	330725.619598	51.676839
3360.207830	330526.651023	51.681844
3359.576847	330323.919673	51.686849
3358.925511	330116.124657	51.691853
3358.003955	329923.418050	51.696858
3357.560189	329716.734752	51.701863
3356.931997	329524.286237	51.706868
3356.291973	329311.344444	51.711873
3355.666946	329104.662657	51.716877
3354.722719	328904.141016	51.721882
3354.523618	328702.839086	51.726887
3353.748841	328505.115593	51.731892
3353.088766	328299.277317	51.736897
3352.352564	328099.815428	51.741901
3351.726928	327893.461427	51.746906
3351.150392	327687.048192	51.751911
3350.276372	327486.664499	51.756916
3349.643614	327280.411832	51.761921
3348.954282	327071.697950	51.766925
3348.041133	326875.825287	51.771930
3347.527588	326673.523936	51.776935
3347.108222	326479.074357	51.781940
3346.405615	326273.492060	51.786945
3345.829038	326072.854056	51.791949
3344.814023	325872.004809	51.796954
3344.163180	325679.346646	51.801959
3343.347332	325470.266658	51.806964
3342.818270	325269.466375	51.811969
3342.232257	325070.558684	51.816973
3341.444218	324872.904562	51.821978
3340.938737	324676.070951	51.826983
3340.145581	324479.256893	51.831988
3339.633586	324280.335583	51.836993
3339.091244	324071.972604	51.841997
3337.897427	323885.150234	51.847002
3337.283735	323674.684286	51.852007
3336.429679	323487.043475	51.857012
3336.316533	323289.100644	51.862017
3335.505738	323089.459917	51.867021
3335.047198	322895.237190	51.872026
3334.117430	322686.295513	51.877031
3333.584203	322498.805479	51.882036
3332.671932	322293.602900	51.887041
3332.249068	322093.211052	51.892045
3331.576389	321893.443858	51.897050
3331.199320	321689.173684	51.902055
3330.176900	321499.110836	51.907060
3329.464095	321289.622254	51.912065
3328.768420	321099.532339	51.917069
3328.128787	320897.593405	51.922074
3327.546611	320699.922525	51.927079
3326.588103	320513.208424	51.932084
3325.984127	320314.572586	51.937089
3325.410829	320114.174579	51.942093
3324.110401	319923.464856	51.947098
3323.727052	319720.566119	51.952103
3323.182803	319535.999707	51.957108
3322.657325	319338.113191	51.962113
3322.173636	319149.335152	51.967117
3321.288955	318957.259102	51.972122
3320.946031	318755.472192	51.977127
3320.157204	318567.428708	51.982132
3319.647235	318363.070193	51.987137
3319.158036	318165.659238	51.992141
3317.812460	317976.709570	51.997146
3317.829361	317769.440108	52.002151
3317.070950	317567.461733	52.007156
3316.009857	317379.509871	52.012161
3315.378400	317184.818440	52.017165
3314.809208	316983.954750	52.022170
3313.937535	316792.406990	52.027175
3313.331686	316589.791341	52.032180
3312.315059	316403.154638	52.037185
3312.105481	316208.445477	52.042189
3311.013877	316020.190270	52.047194
3310.808244	315818.248186	52.052199
3310.231375	315632.202540	52.057204
3309.487652	315434.495281	52.062209
3308.865925	315249.678260	52.067213
3308.221003	315056.563506	52.072218
3307.665465	314851.440969	52.077223
3306.556174	314659.824849	52.082228
3306.276359	314461.991420	52.087233
3305.502550	314265.203346	52.092237
3304.540570	314077.102292	52.097242
3304.411988	313878.709103	52.102247
3303.434103	313681.977666	52.107252
3302.762260	313491.919904	52.112257
3302.101990	313290.630426	52.117261
3301.119989	313102.683586	52.122266
3300.492007	312897.823321	52.127271
3299.979067	312718.892253	52.132276
3299.161801	312523.788444	52.137281
3298.941744	312330.525114	52.142285
3298.009382	312139.818636	52.147290
3297.066312	311938.902400	52.152295
3296.475243	311752.444722	52.157300
3296.023209	311558.707440	52.162305
3295.779487	311367.941664	52.167309
3294.454696	311179.383666	52.172314
3294.038266	310978.306030	52.177319
3293.262145	310793.964102	52.182324
3292.631712	310610.515558	52.187329
3291.865040	310410.612744	52.192333
3291.108203	310226.037674	52.197338
3290.746993	310038.904219	52.202343
3290.010577	309842.917185	52.207348
3289.459631	309656.169627	52.212353
3288.878112	309467.898727	52.217357
3288.042701	309279.005595	52.222362
3287.860602	309082.420346	52.227367
3286.924585	308886.055859	52.232372
3285.984398	308685.948378	52.237377
3285.668104	308496.895530	52.242381
3284.764583	308305.465154	52.247386
3283.927828	308109.211040	52.252391
3282.960084	307925.709838	52.257396
3282.674255	307736.472748	52.262401
3281.718618	307549.123853	52.267405
3281.081617	307357.471612	52.272410
3280.648507	307156.568444	52.277415
3279.703066	306970.795919	52.282420
3278.997623	306793.465096	52.287425
3278.785212	306603.807260	52.292429
3278.097300	306414.402600	52.297434
3277.351679	306214.234945	52.302439
3276.653875	306035.424888	52.307444
3276.046298	305840.786288	52.312449
3275.273134	305658.447943	52.317453
3274.134008	305471.583435	52.322458
3273.985166	305282.575745	52.327463
3273.344789	305088.552410	52.332468
3272.550133	304902.294742	52.337473
3271.953057	304711.294429	52.342477
3270.813287	304533.010653	52.347482
3270.320592	304351.950414	52.352487
3269.760220	304162.013099	52.357492
3269.086037	303967.000369	52.362497
3268.714547	303786.123957	52.367501
3267.904374	303605.800543	52.372506
3267.797548	303409.806018	52.377511
3266.859616	303227.923448	52.382516
3266.340595	303038.309152	52.387521
3265.410394	302846.620494	52.392525
3264.799591	302658.853771	52.397530
3264.185957	302459.016353	52.402535
3263.478202	302277.783788	52.407540
3262.749547	302087.310112	52.412545
3262.499046	301905.699191	52.417549
3261.273679	301707.434555	52.422554
3260.713971	301510.897956	52.427559
3259.968277	301332.420613	52.432564
3259.440381	301138.679795	52.437569
3258.746104	300943.997331	52.442573
3257.822789	300748.892455	52.447578
3257.336047	300567.088133	52.452583
3256.602492	300388.505935	52.457588
3256.014126	300200.809068	52.462593
3255.418746	300000.456271	52.467597
3254.566903	299827.392916	52.472602
3254.164135	299632.306232	52.477607
3253.744361	299444.734636	52.482612
3252.747640	299253.281292	52.487617
3251.727223	299073.826242	52.492621
3251.094488	298882.900645	52.497626
3250.382648	298697.284407	52.502631
3249.595909	298525.711951	52.507636
3248.911037	298335.125060	52.512641
3248.834368	298155.799929	52.517645
3247.971229	297982.303553	52.522650
3247.335239	297783.126041	52.527655
3246.968598	297598.803788	52.532660
3246.072514	297412.935206	52.537665
3245.438870	297230.361085	52.542669
3244.993399	297033.317301	52.547674
3244.415051	296834.944578	52.552679
3243.417320	296658.361267	52.557684
3242.896322	296469.401852	52.562689
3242.394693	296275.014718	52.567693
3241.041826	296095.914888	52.572698
3240.649526	295897.639099	52.577703
3239.628201	295714.055218	52.582708
3238.930914	295523.492871	52.587713
3238.116511	295355.563652	52.592717
3237.773911	295171.999261	52.597722
3237.300652	294982.496055	52.602727
3236.238893	294816.795687	52.607732
3235.836289	294627.866724	52.612737
3235.405168	294441.870829	52.617741
3234.164038	294265.400293	52.622746
3233.665597	294076.944403	52.627751
3233.106430	293905.611964	52.632756
3232.500573	293723.845181	52.637761
3232.100200	293538.480322	52.642765
3231.150895	293350.986469	52.647770
3230.463500	293166.914595	52.652775
3229.826036	292994.040322	52.657780
3228.850359	292809.402536	52.662785
3228.577995	292627.709454	52.667789
3227.427127	292457.437254	52.672794
3226.942021	292272.110231	52.677799
3226.311184	292089.225523	52.682804
3225.917302	291916.719405	52.687809
3225.131119	291736.380282	52.692813
3224.454961	291558.621312	52.697818
3223.891763	291377.737306	52.702823
3223.512738	291190.915562	52.707828
3222.535016	291011.344767	52.712833
3221.950199	290823.587533	52.717837
3221.123606	290647.252434	52.722842
3220.721878	290467.157208	52.727847
3219.855679	290285.403523	52.732852
3219.298051	290104.925227	52.737857
3218.591059	289927.373754	52.742861
3217.751765	289748.926253	52.747866
3217.382063	289560.599287	52.752871
3216.524810	289381.059279	52.757876
3215.678866	289205.159260	52.762881
3215.373420	289020.794744	52.767885
3214.522109	288846.117809	52.772890
3213.781808	288668.112398	52.777895
3213.037852	288488.732196	52.782900
3212.613175	288305.073726	52.787905
3212.041103	288128.289313	52.792909
3210.920502	287951.413286	52.797914
3210.626072	287766.740650	52.802919
3209.761802	287590.358704	52.807924
3209.154293	287409.402761	52.812929
3208.515972	287226.057608	52.817933
3207.912956	287062.215212	52.822938
3207.139472	286882.329422	52.827943
3206.102368	286700.447799	52.832948
3205.715242	286530.407754	52.837953
3205.009068	286348.600945	52.842957
3204.276077	286172.197503	52.847962
3204.005525	285991.645947	52.852967
3203.083063	285821.715715	52.857972
3202.602559	285642.801686	52.862977
3201.899174	285463.719083	52.867981
3201.457189	285288.109645	52.872986
3200.612362	285100.619321	52.877991
3199.895215	284928.567844	52.882996
3199.277506	284750.566499	52.888001
3198.738635	284564.479218	52.893005
3197.339472	284400.277708	52.898010
3197.302299	284209.042762	52.903015
3196.661274	284040.595361	52.908020
3195.876064	283864.122769	52.913025
3195.178432	283681.422026	52.918029
3194.339766	283508.574234	52.923034
3193.624326	283331.479171	52.928039
3193.130736	283155.469552	52.933044
3192.425600	282976.615428	52.938049
3192.069235	282807.231181	52.943053
3191.016646	282634.544267	52.948058
3190.504572	282445.039179	52.953063
3189.977839	282275.859991	52.958068
3188.691903	282095.645755	52.963073
3188.382776	281923.910686	52.968077
3187.619593	281765.108857	52.973082
3187.317074	281575.188311	52.978087
3186.377283	281412.212064	52.983092
3185.727665	281239.893956	52.988097
3185.078352	281058.942009	52.993101
3184.310933	280890.233472	52.998106
3183.809380	280701.821318	53.003111
3182.946449	280535.037926	53.008116
3182.378579	280367.851268	53.013121
3181.843884	280191.923695	53.018125
3180.772095	280030.852665	53.023130
3180.410058	279846.849717	53.028135
3179.583780	279677.411642	53.033140
3179.172307	279499.121345	53.038145
3178.487602	279329.075037	53.043149
3177.481954	279169.113993	53.048154
3176.895550	278982.242972	53.053159
3176.232769	278817.999891	53.058164
3175.783214	278655.913334	53.063169
3174.999234	278470.245021	53.068173
3174.261943	278310.088589	53.073178
3173.872923	278136.811775	53.078183
3173.088562	277967.468668	53.083188
3172.525949	277793.022257	53.088193
3172.055199	277616.523824	53.093197
3171.144991	277443.507650	53.098202
3170.800729	277263.449065	53.103207
3170.377613	277089.642689	53.108212
3169.404119	276911.262648	53.113217
3168.701443	276730.165571	53.118221
3167.945544	276557.379594	53.123226
3167.618254	276370.492723	53.128231
3166.360294	276217.447740	53.133236
3165.921945	276027.751426	53.138241
3165.418200	275856.631905	53.143245
3164.208278	275684.299732	53.148250
3163.938577	275505.782811	53.153255
3163.196716	275342.596145	53.158260
3162.086520	275170.783022	53.163265
3161.762078	275004.143024	53.168269
3161.215499	274831.909652	53.173274
3160.658593	274651.426156	53.178279
3159.702020	274485.268186	53.183284
3159.091402	274310.701860	53.188289
3158.629697	274138.200391	53.193293
3157.496474	273964.862827	53.198298
3157.193282	273792.463638	53.203303
3156.303765	273644.250305	53.208308
3155.777536	273468.269905	53.213313
3155.165923	273292.099278	53.218317
3154.591334	273121.474914	53.223322
3154.058787	272947.533023	53.228327
3153.138551	272785.520742	53.233332
3152.440753	272607.249932	53.238337
3151.697223	272431.609617	53.243341
3150.753544	272261.120127	53.248346
3149.969104	272098.424255	53.253351
3149.560714	271937.655444	53.258356
3148.577155	271768.496679	53.263361
3148.244222	271605.984124	53.268365
3147.586966	271440.543100	53.273370
3147.208018	271276.688047	53.278375
3146.340897	271105.346148	53.283380
3145.571712	270942.851767	53.288385
3145.536089	270758.797024	53.293389
3144.374864	270601.662134	53.298394
3143.811081	270434.245424	53.303399
3143.068578	270267.824816	53.308404
3142.623887	270098.581080	53.313409
3142.159735	269925.494741	53.318413
3141.021323	269760.257473	53.323418
3140.458595	269577.432444	53.328423
3139.836793	269421.231174	53.333428
3138.823677	269246.041562	53.338433
3138.411872	269073.532909	53.343437
3137.692980	268913.526868	53.348442
3137.092806	268749.732781	53.353447
3136.489502	268581.253068	53.358452
3135.639796	268413.831112	53.363457
3135.318707	268241.613947	53.368461
3134.317546	268079.182352	53.373466
3133.924648	267901.322695	53.378471
3132.875637	267740.350455	53.383476
3132.147041	267579.378508	53.388481
3131.739392	267409.416489	53.393485
3131.136795	267247.456914	53.398490
3130.342357	267083.133728	53.403495
3129.615709	266917.348183	53.408500
3129.138850	266747.881225	53.413505
3128.552701	266586.173940	53.418509
3127.678893	266415.114466	53.423514
3127.017395	266244.963786	53.428519
3126.467871	266090.662109	53.433524
3126.157656	265913.961599	53.438529
3125.428488	265747.005328	53.443533
3124.167160	265582.119824	53.448538
3124.007612	265417.976926	53.453543
3123.232093	265256.503820	53.458548
3122.545404	265084.320127	53.463553
3121.877259	264918.627931	53.468557
3121.104336	264751.984593	53.473562
3120.516407	264581.721062	53.478567
3119.725588	264420.199775	53.483572
3119.001836	264259.559326	53.488577
3118.338794	264085.538628	53.493581
3117.614888	263932.691559	53.498586
3117.242723	263758.726867	53.503591
3116.416842	263601.948529	53.508596
3115.659926	263441.288216	53.513601
3115.517714	263266.625216	53.518605
3114.427430	263107.444004	53.523610
3114.079607	262936.226406	53.528615
3113.302392	262773.022822	53.533620
3112.412632	262605.558514	53.538625
3111.942891	262443.656246	53.543629
3111.334571	262269.780608	53.548634
3110.420944	262107.694058	53.553639
3109.810758	261953.632895	53.558644
3109.185132	261780.218686	53.563649
3108.458702	261616.192685	53.568653
3107.860239	261465.135116	53.573658
3107.370655	261284.288529	53.578663
3106.289881	261120.242457	53.583668
3105.316438	260959.566711	53.588673
3104.931389	260793.245989	53.593677
3104.175875	260630.574929	53.598682
3103.821796	260471.405932	53.603687
3102.959805	260316.672365	53.608692
3102.374951	260151.325938	53.613697
3101.684355	259990.911606	53.618701
3101.190218	259832.096216	53.623706
3100.422182	259655.114879	53.628711
3099.786279	259504.268024	53.633716
3099.084996	259349.382246	53.638721
3098.274246	259178.673024	53.643725
3097.638882	259018.225075	53.648730
3097.058366	258849.491585	53.653735
3096.517412	258698.146295	53.658740
3096.015149	258537.219176	53.663745
3094.973272	258368.457136	53.668749
3094.216313	258213.733669	53.673754
3093.643304	258052.512452	53.678759
3093.103564	257894.953396	53.683764
3092.269290	257729.775338	53.688769
3091.692415	257565.626303	53.693773
3091.305617	257413.977284	53.698778
3090.858641	257247.897862	53.703783
3089.813837	257089.298694	53.708788
3088.976971	256929.342433	53.713793
3088.496242	256761.613327	53.718797
3087.513447	256605.271283	53.723802
3086.842081	256454.202744	53.728807
3086.511406	256291.721987	53.733812
3085.767954	256137.991006	53.738817
3084.992901	255978.713270	53.743821
3084.484867	255813.408601	53.748826
3083.780486	255647.014568	53.753831
3082.964808	255502.794748	53.758836
3082.362505	255332.615667	53.763841
3081.900219	255167.788144	53.768845
3080.927986	255013.126429	53.773850
3080.434449	254851.029090	53.778855
3079.795583	254688.496468	53.783860
3079.405411	254532.597004	53.788865
3078.419772	254369.992173	53.793869
3077.700551	254212.311396	53.798874
3077.138317	254050.607583	53.803879
3076.600595	253893.254884	53.808884
3075.739886	253731.853233	53.813889
3075.207356	253571.673140	53.818893
3074.296277	253415.576855	53.823898
3073.474775	253268.965688	53.828903
3073.000498	253109.795445	53.833908
3072.551063	252946.928711	53.838913
3071.777255	252794.070985	53.843917
3071.452204	252637.602491	53.848922
3071.045010	252474.856825	53.853927
3069.886065	252312.841457	53.858932
3069.171168	252140.518334	53.863937
3068.951984	251978.278170	53.868941
3067.713295	251829.009231	53.873946
3067.165705	251670.335722	53.878951
3066.619549	251517.035597	53.883956
3066.092971	251342.875323	53.888961
3065.319990	251189.458580	53.893965
3064.484615	251034.421984	53.898970
3064.217087	250868.141316	53.903975
3063.501758	250707.839908	53.908980
3062.783563	250545.603651	53.913985
3062.285173	250368.358466	53.918989
3061.560688	250216.921322	53.923994
3061.051325	250048.769751	53.928999
3060.243970	249888.407298	53.934004
3059.444322	249710.089970	53.939009
3058.659838	249548.399983	53.944013
3057.817581	249392.551094	53.949018
3057.563745	249231.948912	53.954023
3056.724594	249068.892880	53.959028
3055.498421	248915.931969	53.964033
3055.322592	248742.100948	53.969037
3054.334294	248589.484711	53.974042
3053.793212	248439.904736	53.979047
3053.243447	248281.489519	53.984052
3052.531197	248126.054250	53.989057
3051.823506	247963.717101	53.994061
3051.113246	247815.335951	53.999066
3050.555941	247653.280933	54.004071
3049.899164	247499.289099	54.009076
3049.222120	247342.703099	54.014081
3048.703112	247181.712109	54.019085
3048.143460	247021.975559	54.024090
3047.005030	246865.030156	54.029095
3046.383699	246710.778882	54.034100
3046.147921	246553.028871	54.039105
3045.503018	246398.679798	54.044109
3044.330387	246245.203839	54.049114
3043.743687	246082.493112	54.054119
3043.092371	245934.741198	54.059124
3041.926062	245779.889595	54.064129
3041.324348	245622.351321	54.069133
3040.790642	245474.886871	54.074138
3040.615941	245322.017983	54.079143
3039.711466	245173.288314	54.084148
3039.331718	245018.160305	54.089153
3038.651886	244858.980003	54.094157
3037.926526	244710.349824	54.099162
3037.508203	244553.980640	54.104167
3036.661015	244394.521783	54.109172
3035.731793	244238.717658	54.114177
3035.546619	244077.855685	54.119181
3034.641941	243935.773892	54.124186
3034.422202	243768.220369	54.129191
3033.483087	243612.978788	54.134196
3032.589750	243458.137593	54.139201
3032.265066	243300.048905	54.144205
3031.017810	243151.757726	54.149210
3030.613210	242984.692846	54.154215
3030.090802	242837.153145	54.159220
3029.447343	242677.613226	54.164225
3028.896548	242503.976642	54.169229
3028.194834	242345.999733	54.174234
3027.313960	242183.645924	54.179239
3026.658602	242030.220322	54.184244
3026.027878	241867.750945	54.189249
3025.488154	241710.665950	54.194253
3024.468734	241557.196689	54.199258
3024.100264	241397.003743	54.204263
3023.282450	241245.336443	54.209268
3022.194242	241093.075502	54.214273
3021.810665	240938.818854	54.219277
3020.698508	240793.335716	54.224282
3020.367209	240646.583273	54.229287
3019.812555	240496.454089	54.234292
3019.087245	240337.872373	54.239297
3018.844673	240186.752004	54.244301
3017.737390	240040.836123	54.249306
3017.170250	239885.769566	54.254311
3016.800892	239733.243833	54.259316
3016.025629	239583.150732	54.264321
3015.343068	239423.290273	54.269325
3014.220178	239263.372397	54.274330
3014.027736	239119.248202	54.279335
3013.439880	238969.839252	54.284340
3012.327141	238815.929985	54.289345
3012.118661	238654.645973	54.294349
3010.976722	238510.443637	54.299354
3010.477248	238352.796568	54.304359
3009.938872	238213.260908	54.309364
3008.951221	238066.513777	54.314369
3008.704471	237921.763111	54.319373
3007.766624	237759.882827	54.324378
3007.323175	237604.697974	54.329383
3006.764235	237462.416405	54.334388
3005.923596	237310.961644	54.339393
3005.608149	237149.060162	54.344397
3004.750880	236995.800537	54.349402
3004.180935	236848.225028	54.354407
3003.120140	236687.358896	54.359412
3002.899281	236538.582698	54.364417
3002.155329	236380.136876	54.369421
3001.489963	236235.811214	54.374426
3000.569622	236077.648399	54.379431
2999.943914	235932.298331	54.384436
2999.233300	235778.024178	54.389441
2999.004508	235623.062876	54.394445
2997.679189	235477.976944	54.399450
2997.489764	235320.539903	54.404455
2996.766500	235163.467685	54.409460
2995.976955	235018.883270	54.414465
2995.198150	234866.200006	54.419469
2994.735678	234731.749587	54.424474
2994.123061	234566.614363	54.429479
2993.164797	234413.858330	54.434484
2992.589451	234270.157762	54.439489
2992.362635	234118.508654	54.444493
2991.380880	233971.842714	54.449498
2990.658287	233816.325740	54.454503
2989.721986	233669.907684	54.459508
2988.928591	233521.175557	54.464513
2988.503213	233369.508093	54.469517
2987.624493	233223.183442	54.474522
2987.467911	233076.948427	54.479527
2986.808823	232937.057027	54.484532
2986.017000	232790.999366	54.489537
2985.654945	232630.716590	54.494541
2984.566559	232481.752647	54.499546
2983.705230	232327.966010	54.504551
2983.233599	232191.763583	54.509556
2982.701178	232032.094413	54.514561
2982.380511	231890.775996	54.519565
2981.234188	231747.984321	54.524570
2980.966329	231578.165409	54.529575
2979.917736	231446.231221	54.534580
2979.071130	231290.916190	54.539585
2978.497958	231141.516344	54.544589
2977.694368	230998.926194	54.549594
2977.079817	230854.447594	54.554599
2976.412505	230705.750833	54.559604
2975.740211	230571.517653	54.564609
2975.337785	230423.466905	54.569613
2974.719140	230282.070779	54.574618
2974.361615	230133.198606	54.579623
2973.428720	229979.299861	54.584628
2972.469821	229834.037124	54.589633
2972.212983	229680.846674	54.594637
2971.510235	229540.661729	54.599642
2971.016507	229388.400438	54.604647
2970.073268	229244.562042	54.609652
2969.306562	229079.460776	54.614657
2968.709892	228939.361835	54.619661
2967.826652	228796.965990	54.624666
2967.004040	228655.044552	54.629671
2966.635195	228500.753544	54.634676
2965.658159	228362.956345	54.639681
2965.432501	228214.677582	54.644685
2964.463518	228072.856638	54.649690
2963.949165	227931.167663	54.654695
2963.302445	227787.182878	54.659700
2962.540913	227634.406858	54.664705
2962.291616	227484.274402	54.669709
2961.586741	227349.287413	54.674714
2961.097099	227191.529653	54.679719
2960.081180	227049.284984	54.684724
2959.481906	226906.923686	54.689729
2959.076596	226755.798756	54.694733
2958.221681	226611.416064	54.699738
2957.455906	226448.789398	54.704743
2956.732689	226308.982100	54.709748
2956.047192	226166.037367	54.714753
2955.505313	226014.617122	54.719757
2954.761871	225869.046865	54.724762
2953.942561	225721.630230	54.729767
2953.638291	225579.466374	54.734772
2952.875970	225433.632532	54.739777
2951.938046	225281.958053	54.744781
2951.501071	225149.338242	54.749786
2951.099448	224987.649771	54.754791
2950.195789	224841.852084	54.759796
2949.264466	224695.906274	54.764801
2949.089704	224548.440654	54.769805
2947.856445	224410.996022	54.774810
2947.325581	224264.923955	54.779815
2946.653782	224122.031541	54.784820
2945.695512	223980.534119	54.789825
2945.416932	223842.812054	54.794829
2944.340611	223697.463863	54.799834
2944.209577	223549.063861	54.804839
2943.421957	223415.280319	54.809844
2942.483014	223271.540612	54.814849
2942.130134	223124.589554	54.819853
2941.262452	222993.454510	54.824858
2940.823169	222840.534567	54.829863
2939.837556	222702.862749	54.834868
2939.370609	222562.983184	54.839873
2938.587843	222421.893599	54.844877
2937.814382	222281.782998	54.849882
2937.583234	222127.482146	54.854887
2936.615708	221996.351859	54.859892
2935.837199	221855.746368	54.864897
2935.712901	221709.092779	54.869901
2934.675008	221570.323766	54.874906
2934.143402	221428.610680	54.879911
2933.465885	221280.683400	54.884916
2932.729487	221142.860361	54.889921
2932.260774	220996.911872	54.894925
2931.239628	220855.417371	54.899930
2930.860428	220710.728230	54.904935
2930.364268	220570.589612	54.909940
2929.379182	220434.131110	54.914945
2929.204545	220276.489928	54.919949
2927.914731	220137.763429	54.924954
2927.304079	220000.966404	54.929959
2926.639667	219858.984521	54.934964
2925.983922	219719.572886	54.939969
2925.533985	219575.355407	54.944973
2924.900487	219444.940463	54.949978
2924.214887	219289.877221	54.954983
2923.498417	219158.992204	54.959988
2922.501542	219026.038740	54.964993
2922.308627	218872.884170	54.969997
2921.618016	218731.086829	54.975002
2920.796333	218590.125184	54.980007
2920.234369	218460.604455	54.985012
2919.386111	218305.301749	54.990017
2918.825024	218161.906604	54.995021
2917.928014	218032.770638	55.000026
2917.508647	217873.047612	55.005031
2916.916020	217738.530499	55.010036
2915.822831	217605.938590	55.015041
2915.386138	217462.436056	55.020045
2914.670720	217332.547061	55.025050
2914.165295	217193.371088	55.030055
2913.368230	217049.086323	55.035060
2912.877537	216912.708945	55.040065
2912.256142	216773.475786	55.045069
2911.274778	216641.644454	55.050074
2910.597000	216494.312473	55.055079
2910.133312	216355.958931	55.060084
2909.542733	216211.490463	55.065089
2908.941222	216074.801314	55.070093
2907.982998	215933.688378	55.075098
2907.596576	215802.579104	55.080103
2906.753693	215661.868514	55.085108
2906.140098	215524.049515	55.090113
2905.726927	215383.258746	55.095117
2904.902150	215244.009944	55.100122
2904.456884	215107.285258	55.105127
2904.032862	214964.740522	55.110132
2902.904957	214827.169816	55.115137
2902.523923	214664.698719	55.120141
2901.613188	214535.825996	55.125146
2900.994693	214391.034852	55.130151
2899.997964	214250.606107	55.135156
2899.159855	214124.713861	55.140161
2898.795684	213983.790961	55.145165
2898.264065	213857.417935	55.150170
2897.659766	213706.210925	55.155175
2896.714534	213565.635457	55.160180
2895.933171	213426.612654	55.165185
2895.189436	213296.493972	55.170189
2894.682328	213159.999425	55.175194
2894.113931	213018.449034	55.180199
2893.429435	212895.258641	55.185204
2892.722896	212747.722997	55.190209
2892.245477	212615.221523	55.195213
2891.481206	212484.242187	55.200218
2890.947250	212349.535512	55.205223
2890.411187	212218.024190	55.210228
2889.270035	212072.468083	55.215233
2888.696951	211934.293712	55.220237
2888.155207	211802.618669	55.225242
2887.544758	211660.810597	55.230247
2886.925766	211527.557352	55.235252
2886.256616	211391.219445	55.240257
2885.681147	211243.501015	55.245261
2884.715567	211112.556330	55.250266
2884.302863	210972.436736	55.255271
2883.951853	210833.618644	55.260276
2883.105363	210697.997592	55.265281
2882.629199	210551.105080	55.270285
2881.925388	210422.131360	55.275290
2881.109284	210273.129599	55.280295
2880.477396	210135.617543	55.285300
2879.721600	209994.421667	55.290305
2879.228686	209852.217197	55.295309
2878.369313	209715.454818	55.300314
2878.094217	209578.383876	55.305319
2877.164944	209430.178416	55.310324
2876.292358	209296.511831	55.315329
2875.840267	209142.058694	55.320333
2875.059174	209007.856422	55.325338
2874.541226	208869.094564	55.330343
2873.591990	208734.232228	55.335348
2872.940931	208594.448418	55.340353
2872.853854	208451.177455	55.345357
2871.704891	208318.333110	55.350362
2871.042466	208173.193881	55.355367
2870.296809	208033.044512	55.360372
2869.796284	207899.296612	55.365377
2868.999152	207761.841453	55.370381
2868.547716	207625.897314	55.375386
2867.814880	207481.407240	55.380391
2866.987507	207344.606898	55.385396
2866.447909	207211.719417	55.390401
2866.079863	207063.659933	55.395405
2864.972052	206938.219220	55.400410
2864.577528	206795.140840	55.405415
2863.931845	206651.682575	55.410420
2862.901997	206510.436317	55.415425
2862.440382	206373.007581	55.420429
2861.588730	206247.947755	55.425434
2860.999574	206102.331032	55.430439
2860.396910	205982.832139	55.435444
2859.655401	205839.009206	55.440449
2859.317002	205696.268210	55.445453
2858.057375	205566.247366	55.450458
2857.798558	205429.068707	55.455463
2857.433903	205290.978081	55.460468
2856.644895	205146.986190	55.465473
2855.837277	205000.452289	55.470477
2855.249342	204875.620893	55.475482
2854.838666	204725.066891	55.480487
2853.824887	204582.181009	55.485492
2852.720163	204455.994242	55.490497
2852.703092	204319.645322	55.495501
2851.869772	204180.091638	55.500506
2851.668114	204043.556246	55.505511
2850.676306	203903.188387	55.510516
2849.998251	203761.205866	55.515521
2849.278257	203629.436795	55.520525
2848.603148	203484.883790	55.525530
2847.927677	203347.788759	55.530535
2847.235337	203214.298234	55.535540
2846.706085	203072.777464	55.540545
2845.956393	202931.444660	55.545549
2845.477212	202796.266979	55.550554
2844.704743	202653.691321	55.555559
2843.885139	202527.323697	55.560564
2843.172502	202383.835703	55.565569
2842.930184	202242.424300	55.570573
2841.738126	202112.553313	55.575578
2841.185657	201965.465050	55.580583
2840.700494	201840.636762	55.585588
2839.676085	201707.762325	55.590593
2839.362486	201567.700127	55.595597
2838.615681	201427.083306	55.600602
2837.834354	201288.584779	55.605607
2837.434252	201145.954020	55.610612
2836.355628	201009.933869	55.615617
2835.752732	200879.056245	55.620621
2834.978202	200750.993014	55.625626
2834.799669	200607.081461	55.630631
2833.919396	200474.861630	55.635636
2832.996873	200337.024132	55.640641
2832.687360	200197.702851	55.645645
2831.775366	200069.650255	55.650650
2831.279711	199943.211798	55.655655
2830.782528	199804.035766	55.660660
2830.085648	199663.771878	55.665665
2829.724836	199520.630125	55.670669
2828.711499	199391.195393	55.675674
2828.121711	199251.182852	55.680679
2827.502826	199112.600507	55.685684
2826.695939	198972.788492	55.690689
2826.080421	198833.506450	55.695693
2824.917096	198704.262550	55.700698
2824.520410	198565.939117	55.705703
2823.967511	198435.313987	55.710708
2823.411028	198295.693149	55.715713
2822.714052	198158.779897	55.720717
2821.894923	198031.290086	55.725722
2821.549475	197886.241529	55.730727
2820.994487	197745.629359	55.735732
2820.179240	197609.766970	55.740737
2819.491371	197469.749195	55.745741
2818.915304	197334.740385	55.750746
2818.485174	197198.818082	55.755751
2817.739990	197058.454185	55.760756
2817.020647	196912.195041	55.765761
2816.056988	196767.247456	55.770765
2815.364444	196644.385471	55.775770
2814.859577	196501.274679	55.780775
2814.328497	196355.852562	55.785780
2813.259157	196231.167980	55.790785
2813.061848	196082.525377	55.795789
2811.906121	195951.365660	55.800794
2811.495993	195809.641470	55.805799
2811.097136	195683.465091	55.810804
2810.353718	195540.496527	55.815809
2809.834285	195396.907578	55.820813
2808.851094	195269.094230	55.825818
2808.484684	195119.488692	55.830823
2807.866075	194983.156708	55.835828
2806.559848	194851.769153	55.840833
2805.954189	194712.140282	55.845837
2805.568639	194583.394235	55.850842
2805.125835	194436.016798	55.855847
2804.312627	194300.366389	55.860852
2803.463255	194163.691426	55.865857
2803.059152	194021.042405	55.870861
2802.262080	193891.701633	55.875866
2801.643025	193752.332016	55.880871
2801.090203	193609.211479	55.885876
2800.242223	193479.243639	55.890881
2799.949574	193328.321170	55.895885
2798.987096	193196.845339	55.900890
2798.344741	193054.542166	55.905895
2797.490031	192921.001480	55.910900
2796.819114	192786.236027	55.915905
2796.802244	192635.221099	55.920909
2795.256398	192508.292731	55.925914
2794.627319	192367.859797	55.930919
2794.188752	192230.438017	55.935924
2793.607848	192102.950752	55.940929
2793.168887	191965.504327	55.945933
2792.065976	191831.751421	55.950938
2792.197837	191688.718872	55.955943
2791.357695	191549.479525	55.960948
2790.779884	191416.700646	55.965953
2790.594126	191256.276003	55.970957
2789.550256	191120.912565	55.975962
2788.550223	190965.554429	55.980967
2788.051551	190827.039195	55.985972
2787.544525	190684.250713	55.990977
2786.534288	190531.834626	55.995981
2786.073274	190400.248728	56.000986
2785.287352	190256.067972	56.005991
2784.614002	190115.686712	56.010996
2783.846158	189977.369217	56.016001
2783.384874	189824.257749	56.021005
2782.526564	189692.571304	56.026010
2781.842690	189551.226430	56.031015
2781.276592	189414.570752	56.036020
2780.860640	189271.186807	56.041025
2779.977923	189122.571839	56.046029
2779.034477	188984.450426	56.051034
2778.764952	188837.469537	56.056039
2778.093572	188699.178650	56.061044
2777.057736	188559.330116	56.066049
2776.665001	188419.049378	56.071053
2775.913519	188278.596860	56.076058
2775.265276	188140.393008	56.081063
2774.640713	188003.318107	56.086068
2773.876612	187858.174282	56.091073
2773.381234	187721.664978	56.096077
2772.579451	187584.085032	56.101082
2772.446733	187436.170860	56.106087
2771.615030	187295.644943	56.111092
2770.591245	187156.434807	56.116097
2770.009226	187003.224405	56.121101
2769.396569	186868.848050	56.126106
2768.739111	186726.477009	56.131111
2767.571616	186585.561150	56.136116
2767.265680	186444.254854	56.141121
2766.395289	186305.964419	56.146125
2765.513057	186175.589296	56.151130
2765.380188	186040.465123	56.156135
2764.601987	185913.013023	56.161140
2763.912270	185781.934279	56.166145
2763.538808	185631.964920	56.171149
2762.962822	185487.854666	56.176154
2762.191717	185345.913006	56.181159
2761.327771	185201.047796	56.186164
2760.666317	185058.529920	56.191169
2760.287363	184920.662007	56.196173
2759.253591	184783.559728	56.201178
2758.908807	184632.177044	56.206183
2758.689180	184493.076667	56.211188
2757.564503	184348.255480	56.216193
2757.184555	184198.113798	56.221197
2756.363256	184061.425320	56.226202
2755.598585	183919.207263	56.231207
2755.153870	183774.407467	56.236212
2754.144819	183632.521610	56.241217
2753.705285	183480.509038	56.246221
2752.702416	183346.204915	56.251226
2751.987592	183199.350781	56.256231
2751.762799	183059.950375	56.261236
2750.704584	182924.880310	56.266241
2750.263535	182777.691637	56.271245
2749.659534	182633.493227	56.276250
2749.111978	182483.409316	56.281255
2748.016171	182353.918688	56.286260
2747.405251	182210.816749	56.291265
2746.934651	182061.396292	56.296269
2746.153377	181928.753252	56.301274
2745.721622	181780.675995	56.306279
2745.021665	181637.068484	56.311284
2744.145145	181495.143080	56.316289
2743.716981	181349.788918	56.321293
2743.007700	181212.175652	56.326298
2742.360892	181070.825839	56.331303
2742.110965	180926.907716	56.336308
2741.186299	180776.456899	56.341313
2740.891545	180623.973363	56.346317
2739.580803	180487.335353	56.351322
2739.041910	180340.501122	56.356327
2738.536945	180193.674740	56.361332
2737.884919	180047.101111	56.366337
2737.138462	179901.293423	56.371341
2736.433654	179757.591165	56.376346
2735.937150	179605.486635	56.381351
2735.242844	179472.214083	56.386356
2734.715658	179327.734664	56.391361
2734.144357	179172.361783	56.396365
2733.090987	179022.662541	56.401370
2732.727816	178879.837689	56.406375
2731.977862	178730.600219	56.411380
2730.929727	178595.567530	56.416385
2730.500276	178445.975036	56.421389
2730.214731	178300.901185	56.426394
2729.221558	178147.188832	56.431399
2728.879763	177999.581013	56.436404
2727.868224	177861.174211	56.441409
2727.524400	177703.481204	56.446413
2726.805327	177565.181696	56.451418
2725.978436	177409.703157	56.456423
2725.631259	177261.488264	56.461428
2724.553478	177109.395756	56.466433
2724.228262	176974.304683	56.471437
2723.258598	176825.795629	56.476442
2722.640221	176677.269631	56.481447
2721.791463	176529.263977	56.486452
2721.448889	176386.635154	56.491457
2720.939708	176233.781703	56.496461
2720.050257	176091.660235	56.501466
2719.351230	175946.253063	56.506471
2718.483268	175794.157604	56.511476
2717.806867	175656.480937	56.516481
2717.231999	175511.030206	56.521485
2716.424165	175363.136736	56.526490
2716.010147	175217.203701	56.531495
2715.239306	175082.227565	56.536500
2714.812922	174943.127375	56.541505
2714.318095	174778.601418	56.546509
2713.579067	174631.170295	56.551514
2712.819342	174486.897160	56.556519
2712.257048	174335.598151	56.561524
2711.389203	174194.688120	56.566529
2710.876982	174046.510978	56.571533
2710.189547	173898.667369	56.576538
2709.677856	173739.668033	56.581543
2709.038309	173597.630167	56.586548
2708.016284	173449.039958	56.591553
2707.417468	173297.954122	56.596557
2706.861301	173154.963482	56.601562
2706.443583	173000.276324	56.606567
2705.446352	172851.760715	56.611572
2704.977257	172702.844069	56.616577
2704.607105	172551.941045	56.621581
2704.060553	172407.565320	56.626586
2703.180837	172249.634906	56.631591
2702.502695	172092.169187	56.636596
2701.735845	171937.490589	56.641601
2701.395928	171779.654606	56.646605
2700.577334	171643.845536	56.651610
2699.825607	171490.717835	56.656615
2699.061786	171333.357738	56.661620
2698.662555	171177.657375	56.666625
2697.967190	171016.243577	56.671629
2697.121899	170865.765623	56.676634
2696.856386	170703.649171	56.681639
2696.164920	170554.521514	56.686644
2695.149572	170402.876863	56.691649
2694.812479	170245.809638	56.696653
2694.014057	170090.787254	56.701658
2693.097847	169931.231464	56.706663
2692.748327	169783.604081	56.711668
2691.650991	169626.494453	56.716673
2690.973575	169470.539772	56.721677
2690.421763	169327.969318	56.726682
2689.766127	169169.736100	56.731687
2689.002543	169020.892826	56.736692
2688.337419	168872.034534	56.741697
2687.857742	168711.689806	56.746701
2687.056434	168569.886527	56.751706
2686.546384	168413.579000	56.756711
2685.834272	168255.091458	56.761716
2684.992624	168111.134480	56.766721
2684.808922	167954.840725	56.771725
2683.703636	167813.647925	56.776730
2683.230515	167652.174863	56.781735
2682.965268	167505.382181	56.786740
2681.938171	167355.417257	56.791745
2681.282604	167190.261953	56.796749
2680.586715	167041.085079	56.801754
2679.850653	166886.981362	56.806759
2679.492821	166743.868503	56.811764
2678.619231	166582.577888	56.816769
2678.116213	166415.049387	56.821773
2677.188382	166268.277459	56.826778
2676.622553	166121.982829	56.831783
2675.962223	165973.491215	56.836788
2675.082565	165815.167618	56.841793
2674.643993	165660.309754	56.846797
2673.790677	165514.101191	56.851802
2673.245749	165354.963603	56.856807
2672.701232	165201.472269	56.861812
2671.904327	165051.276675	56.866817
2671.607468	164893.525895	56.871821
2671.008328	164740.095987	56.876826
2670.386730	164580.592415	56.881831
2669.520567	164422.565080	56.886836
2668.798352	164274.535105	56.891841
2668.560548	164121.940594	56.896845
2667.654719	163960.119739	56.901850
2667.161929	163804.744212	56.906855
2666.309530	163646.578175	56.911860
2665.705336	163485.182093	56.916865
2664.973160	163326.591527	56.921869
2664.229534	163172.822334	56.926874
2663.547562	163009.609762	56.931879
2662.819981	162846.583151	56.936884
2662.152480	162702.187255	56.941889
2661.749391	162535.003854	56.946893
2660.999055	162389.554310	56.951898
2660.202312	162220.438552	56.956903
2659.727098	162066.682396	56.961908
2658.962648	161913.188853	56.966913
2658.360984	161753.033368	56.971917
2657.296740	161608.297839	56.976922
2656.727845	161442.366327	56.981927
2656.290533	161293.235405	56.986932
2655.511784	161140.764554	56.991937
2654.941361	160981.548404	56.996941
2654.516467	160824.890826	57.001946
2653.959147	160667.759075	57.006951
2653.130299	160507.263741	57.011956
2652.561336	160345.227750	57.016961
2652.107942	160177.885320	57.021965
2651.117080	160018.536660	57.026970
2650.775037	159852.907174	57.031975
2650.044418	159690.848930	57.036980
2649.120418	159534.225258	57.041985
2648.714498	159368.277616	57.046989
2647.910911	159203.398097	57.051994
2647.337599	159045.487864	57.056999
2646.425444	158896.009995	57.062004
2645.696817	158734.108404	57.067009
2645.158514	158573.919103	57.072013
2644.485054	158420.540688	57.077018
2643.809852	158254.145169	57.082023
2643.362137	158085.146408	57.087028
2642.482634	157932.603690	57.092033
2641.912222	157774.101244	57.097037
2641.023577	157611.620004	57.102042
2640.788935	157446.201009	57.107047
2640.083485	157283.069372	57.112052
2639.044288	157131.330946	57.117057
2638.788970	156962.790257	57.122061
2637.939126	156807.336648	57.127066
2637.161122	156650.168907	57.132071
2636.697622	156485.083156	57.137076
2635.896627	156327.056100	57.142081
2635.266458	156169.562048	57.147085
2634.804412	156014.190437	57.152090
2634.221321	155848.020745	57.157095
2633.621250	155685.032551	57.162100
2632.858158	155516.592116	57.167105
2632.408861	155345.051960	57.172109
2631.303423	155192.925841	57.177114
2630.559311	155025.819572	57.182119
2630.114684	154859.747180	57.187124
2629.502784	154696.549503	57.192129
2628.859334	154528.539929	57.197133
2627.868790	154376.526397	57.202138
2627.766681	154204.542963	57.207143
2626.683818	154048.973619	57.212148
2626.149647	153887.051397	57.217153
2625.487026	153719.303125	57.222157
2624.680336	153556.243522	57.227162
2624.013975	153390.416879	57.232167
2623.496868	153232.727921	57.237172
2622.786347	153079.951376	57.242177
2622.269640	152908.510573	57.247181
2621.433715	152745.307030	57.252186
2620.944669	152583.955962	57.257191
2620.412147	152420.833057	57.262196
2619.658943	152255.712201	57.267201
2619.071398	152087.019659	57.272205
2618.521297	151925.490807	57.277210
2617.783226	151756.251822	57.282215
2617.134253	151580.428294	57.287220
2616.412384	151409.205696	57.292225
2615.864404	151252.624139	57.297229
2615.246868	151098.087987	57.302234
2614.604310	150915.072998	57.307239
2613.938994	150745.878529	57.312244
2612.842872	150587.416915	57.317249
2612.471990	150412.445295	57.322253
2611.660815	150237.531651	57.327258
2610.696860	150079.903130	57.332263
2610.355048	149912.885956	57.337268
2609.767379	149746.963495	57.342273
2609.309013	149581.173914	57.347277
2608.275237	149419.759470	57.352282
2607.691876	149270.501052	57.357287
2607.194008	149024.282005	57.362292
2606.296583	148854.219076	57.367297
2606.314342	148683.554526	57.372301
2605.357560	148517.633302	57.377306
2604.451355	148358.389951	57.382311
2603.982698	148181.298025	57.387316
2603.339715	148013.436039	57.392321
2602.742312	147837.268752	57.397325
2601.803238	147679.635314	57.402330
2600.989656	147508.485981	57.407335
2600.472632	147341.446355	57.412340
2599.815289	147182.220274	57.417345
2599.411364	147009.165963	57.422349
2598.588965	146833.865929	57.427354
2597.913755	146672.294149	57.432359
2597.384228	146499.796271	57.437364
2596.582278	146327.355200	57.442369
2595.943459	146153.249856	57.447373
2595.023822	145989.420088	57.452378
2594.331133	145829.939536	57.457383
2593.868862	145660.777839	57.462388
2592.944383	145501.805872	57.467393
2592.586004	145329.922685	57.472397
2591.735463	145165.400038	57.477402
2590.785116	144999.305588	57.482407
2590.610464	144850.282743	57.487412
2589.629151	144680.395270	57.492417
2589.625748	144502.360696	57.497421
2588.962361	144347.381557	57.502426
2587.694564	144165.711535	57.507431
2587.599612	143999.893535	57.512436
2586.571931	143840.183941	57.517441
2586.093028	143673.729608	57.522445
2585.396251	143499.864255	57.527450
2584.871216	143323.787041	57.532455
2584.033698	143156.528221	57.537460
2583.112733	142986.716714	57.542465
2582.490776	142824.127142	57.547469
2581.838758	142658.874750	57.552474
2581.257529	142492.824209	57.557479
2580.694019	142320.596287	57.562484
2579.838567	142154.883278	57.567489
2579.461198	141990.556682	57.572493
2578.742137	141821.088134	57.577498
2578.216923	141659.734656	57.582503
2577.258708	141483.190260	57.587508
2576.640400	141316.376898	57.592513
2576.428818	141148.839288	57.597517
2575.588021	140981.008399	57.602522
2574.712053	140810.121839	57.607527
2574.093884	140641.241073	57.612532
2573.272142	140465.227339	57.617537
2572.955538	140300.290371	57.622541
2571.969374	140132.347459	57.627546
2571.521005	139967.318835	57.632551
2571.136831	139801.455077	57.637556
2570.094755	139623.079799	57.642561
2569.580338	139450.441116	57.647565
2568.709544	139283.056423	57.652570
2568.116693	139117.191393	57.657575
2567.739681	138946.757287	57.662580
2567.063005	138785.189073	57.667585
2566.478087	138594.169308	57.672589
2565.941978	138422.492887	57.677594
2565.258963	138254.893634	57.682599
2564.600166	138080.659506	57.687604
2563.822979	137907.995153	57.692609
2563.467816	137724.516682	57.697613
2562.340603	137553.154926	57.702618
2561.812863	137377.595583	57.707623
2561.154325	137204.878423	57.712628
2560.391709	137030.209568	57.717633
2559.682805	136853.678393	57.722637
2558.950835	136682.678323	57.727642
2558.455353	136512.111839	57.732647
2557.914477	136337.704165	57.737652
2556.925481	136172.998257	57.742657
2556.272012	135993.897240	57.747661
2555.550023	135819.076712	57.752666
2555.072887	135638.895505	57.757671
2554.251613	135478.664119	57.762676
2553.250285	135308.273734	57.767681
2552.841211	135138.298657	57.772685
2552.272026	134976.149956	57.777690
2551.827835	134798.661899	57.782695
2551.147735	134617.388568	57.787700
2550.192626	134464.031150	57.792705
2549.525570	134286.797501	57.797709
2548.789229	134120.017970	57.802714
2548.245065	133957.553435	57.807719
2547.737952	133784.654714	57.812724
2546.631894	133614.024146	57.817729
2546.207366	133448.723462	57.822733
2545.473320	133284.133321	57.827738
2545.051718	133113.155930	57.832743
2544.594892	132944.217574	57.837748
2543.515373	132770.983768	57.842753
2543.273246	132602.902596	57.847757
2542.495818	132439.594446	57.852762
2541.856927	132262.953158	57.857767
2541.227726	132083.529622	57.862772
2540.371737	131914.076310	57.867777
2540.216120	131735.748540	57.872781
2539.087968	131585.558706	57.877786
2538.636048	131401.716465	57.882791
2538.151862	131216.686550	57.887796
2536.887217	131051.113737	57.892801
2536.334803	130874.950073	57.897805
2535.470200	130706.712033	57.902810
2534.728115	130536.258205	57.907815
2534.397180	130373.196078	57.912820
2533.893124	130205.157944	57.917825
2533.492748	130029.635963	57.922829
2532.397642	129862.023775	57.927834
2532.089809	129683.377477	57.932839
2531.603736	129512.520974	57.937844
2531.026021	129335.926445	57.942849
2530.580563	129159.248574	57.947853
2529.532296	128969.534585	57.952858
2528.734116	128804.015465	57.957863
2528.189807	128630.658835	57.962868
2527.199325	128462.962287	57.967873
2526.809173	128276.997063	57.972877
2525.829447	128112.425284	57.977882
2525.400782	127937.251197	57.982887
2525.251123	127756.204543	57.987892
2523.773447	127576.880840	57.992897
2523.613123	127391.342374	57.997901
2522.985338	127215.569415	58.002906
2522.331672	127050.850712	58.007911
2521.405517	126865.881645	58.012916
2520.851544	126692.830829	58.017921
2520.295085	126512.910915	58.022925
2519.469970	126344.489891	58.027930
2518.683079	126160.722698	58.032935
2518.322877	125980.127515	58.037940
2517.417376	125807.099916	58.042945
2516.993969	125632.777886	58.047949
2516.113396	125457.043598	58.052954
2515.521447	125279.613816	58.057959
2515.223709	125107.662697	58.062964
2514.415897	124929.355076	58.067969
2513.670619	124748.308445	58.072973
2512.907268	124573.374052	58.077978
2512.006952	124390.678135	58.082983
2511.656774	124214.334529	58.087988
2510.651274	124037.067330	58.092993
2510.383178	123864.662283	58.097997
2509.539148	123689.340069	58.103002
2509.098967	123516.075636	58.108007
2508.319631	123335.996287	58.113012
2507.311015	123155.357665	58.118017
2507.129491	122976.963754	58.123021
2506.271383	122802.982882	58.128026
2505.646094	122632.343912	58.133031
2504.952538	122449.996710	58.138036
2504.051085	122272.877099	58.143041
2503.446662	122093.172060	58.148045
2502.687221	121919.930496	58.153050
2502.401579	121742.856513	58.158055
2501.633447	121565.898264	58.163060
2500.820518	121389.862508	58.168065
2500.297544	121219.444967	58.173069
2499.789221	121050.613357	58.178074
2499.263393	120877.646339	58.183079
2498.573753	120681.293086	58.188084
2497.829117	120514.457703	58.193089
2497.427467	120326.695389	58.198093
2496.486937	120158.814077	58.203098
2495.528899	119980.550723	58.208103
2494.983677	119801.956537	58.213108
2494.308516	119617.499329	58.218113
2494.148756	119429.952697	58.223117
2493.347305	119259.763418	58.228122
2492.565447	119086.804364	58.233127
2492.039933	118899.649612	58.238132
2491.368761	118714.182474	58.243137
2490.690834	118527.067255	58.248141
2489.960353	118348.252132	58.253146
2489.233955	118168.263234	58.258151
2488.891271	117988.202087	58.263156
2487.861145	117812.262952	58.268161
2487.255577	117620.667614	58.273165
2486.668511	117443.594358	58.278170
2485.846493	117273.364268	58.283175
2485.283217	117085.911245	58.288180
2484.584557	116912.122018	58.293185
2483.878282	116728.604383	58.298189
2483.164118	116553.918690	58.303194
2482.537928	116371.711203	58.308199
2481.948368	116188.445538	58.313204
2481.055798	116018.171494	58.318209
2480.846600	115830.493826	58.323213
2480.227211	115644.259902	58.328218
2479.368926	115468.360412	58.333223
2478.967992	115289.641329	58.338228
2478.353601	115106.488940	58.343233
2477.574274	114919.219357	58.348237
2476.632811	114730.478949	58.353242
2476.197351	114546.527913	58.358247
2475.830072	114362.510287	58.363252
2474.303140	114192.450581	58.368257
2473.972546	113997.906618	58.373261
2473.150060	113827.902755	58.378266
2472.315803	113651.967668	58.383271
2471.786923	113465.691016	58.388276
2471.301064	113297.446214	58.393281
2470.745759	113111.176382	58.398285
2469.690776	112935.611325	58.403290
2469.506353	112757.364570	58.408295
2468.935163	112572.027866	58.413300
2468.134336	112399.294921	58.418305
2467.811378	112213.236125	58.423309
2466.916959	112025.289216	58.428314
2465.964745	111839.212358	58.433319
2465.641376	111661.922017	58.438324
2464.794562	111479.448528	58.443329
2464.098745	111300.303236	58.448333
2463.331515	111124.889394	58.453338
2462.608919	110938.160990	58.458343
2462.274064	110753.891926	58.463348
2461.406557	110580.915680	58.468353
2460.911227	110392.689460	58.473357
2460.182276	110214.363234	58.478362
2459.380381	110027.705061	58.483367
2458.916422	109841.381844	58.488372
2458.053052	109672.187089	58.493377
2457.673379	109484.533306	58.498381
2456.616731	109296.664620	58.503386
2456.189521	109115.360521	58.508391
2455.809312	108934.786403	58.513396
2454.833687	108765.558601	58.518401
2454.407605	108573.800919	58.523405
2453.554115	108392.817221	58.528410
2452.962012	108221.159231	58.533415
2452.376350	108032.242114	58.538420
2451.497400	107850.447944	58.543425
2450.869356	107666.331086	58.548429
2450.311969	107493.391005	58.553434
2449.752599	107305.319299	58.558439
2449.078184	107117.038865	58.563444
2448.189574	106931.782365	58.568449
2447.400901	106750.870463	58.573453
2446.801055	106577.861186	58.578458
2445.870596	106394.112864	58.583463
2445.557300	106221.682536	58.588468
2444.922947	106039.672903	58.593473
2444.524854	105848.731849	58.598477
2443.398886	105686.642889	58.603482
2442.952649	105503.605049	58.608487
2442.626137	105310.556858	58.613492
2441.500079	105127.991283	58.618497
2440.954803	104950.537567	58.623501
2440.109180	104771.553000	58.628506
2439.640681	104583.488235	58.633511
2439.139689	104402.751517	58.638516
2438.464174	104224.372203	58.643521
2437.907393	104038.730244	58.648525
2437.102864	103856.313808	58.653530
2436.504954	103671.702666	58.658535
2436.304948	103482.785676	58.663540
2435.136339	103307.244778	58.668545
2434.395152	103116.449827	58.673549
2433.807471	102922.618701	58.678554
2433.553159	102749.696680	58.683559
2432.888401	102565.079420	58.688564
2431.996828	102375.754372	58.693569
2431.402740	102177.267691	58.698573
2430.612054	101997.090129	58.703578
2429.597221	101811.297262	58.708583
2429.215197	101626.128748	58.713588
2428.540434	101448.582334	58.718593
2427.803137	101258.842228	58.723597
2427.287907	101072.874557	58.728602
2426.972427	100886.337519	58.733607
2426.103238	100703.822632	58.738612
2425.228213	100522.654890	58.743617
2424.761964	100330.037589	58.748621
2424.006763	100144.324712	58.753626
2423.157124	99959.116716	58.758631
2422.847879	99776.913655	58.763636
2422.322461	99579.529260	58.768641
2421.554400	99398.943267	58.773645
2420.874957	99207.923143	58.778650
2419.689942	99016.204556	58.783655
2419.360535	98835.800827	58.788660
2418.648001	98656.791229	58.793665
2418.120808	98460.253963	58.798669
2417.375056	98283.434453	58.803674
2416.529270	98091.841075	58.808679
2415.975195	97896.651205	58.813684
2414.962031	97729.170285	58.818689
2414.511912	97541.578044	58.823693
2414.056818	97358.402483	58.828698
2413.541316	97164.823741	58.833703
2412.931707	96979.386111	58.838708
2411.756733	96800.096502	58.843713
2411.477036	96604.449274	58.848717
2410.801261	96421.728482	58.853722
2410.124881	96239.928868	58.858727
2409.363989	96056.742508	58.863732
2408.624639	95875.317305	58.868737
2408.152685	95685.834898	58.873741
2407.467296	95507.708272	58.878746
2406.735465	95316.786142	58.883751
2406.277317	95116.404633	58.888756
2405.164174	94944.837951	58.893761
2405.038306	94747.514532	58.898765
2404.119505	94559.767620	58.903770
2403.508472	94376.571171	58.908775
2403.052964	94185.969983	58.913780
2402.096049	94005.348998	58.918785
2401.573645	93811.692309	58.923789
2400.691533	93634.055639	58.928794
2400.102068	93446.348309	58.933799
2399.688592	93248.988568	58.938804
2398.572212	93073.670025	58.943809
2398.233436	92888.191491	58.948813
2397.641382	92698.176344	58.953818
2396.778676	92513.069341	58.958823
2396.003088	92320.404241	58.963828
2395.337589	92139.143475	58.968833
2394.806724	91947.730047	58.973837
2394.181093	91774.854999	58.978842
2393.587118	91590.911541	58.983847
2393.301819	91401.340808	58.988852
2392.346794	91213.608879	58.993857
2391.514280	91027.837420	58.998861
2390.741258	90840.720232	59.003866
2390.515186	90658.964479	59.008871
2389.798905	90454.037312	59.013876
2389.050485	90267.802438	59.018881
2388.554074	90089.885840	59.023885
2387.907224	89905.451302	59.028890
2386.948875	89713.446674	59.033895
2386.627010	89520.543976	59.038900
2385.523119	89331.501307	59.043905
2385.015079	89136.843586	59.048909
2384.564194	88948.746849	59.053914
2383.769924	88765.765496	59.058919
2383.013048	88572.401254	59.063924
2382.442116	88385.526674	59.068929
2381.692673	88187.790154	59.073933
2381.053800	88014.465108	59.078938
2380.435961	87826.157319	59.083943
2379.870282	87631.344734	59.088948
2378.977729	87452.288965	59.093953
2378.565883	87250.722751	59.098957
2377.662061	87069.377028	59.103962
2377.122400	86877.052224	59.108967
2376.406073	86694.215530	59.113972
2375.671410	86507.909337	59.118977
2375.279774	86308.878147	59.123981
2374.286387	86124.492728	59.128986
2373.902133	85936.164457	59.133991
2373.788255	85743.902765	59.138996
2372.698355	85559.486804	59.144001
2372.041572	85349.616058	59.149005
2371.327291	85167.483037	59.154010
2370.320920	84980.320421	59.159015
2369.805636	84786.127902	59.164020
2369.406140	84599.043589	59.169025
2368.793354	84395.057671	59.174029
2367.850946	84221.038114	59.179034
2367.143119	84034.793648	59.184039
2366.564858	83835.403138	59.189044
2365.719682	83655.991385	59.194049
2365.127218	83456.879252	59.199053
2364.196217	83271.874852	59.204058
2363.509039	83085.635481	59.209063
2363.010274	82902.099684	59.214068
2362.226069	82719.111455	59.219073
2361.615361	82533.295849	59.224077
2360.877824	82345.873100	59.229082
2360.244701	82157.776316	59.234087
2359.992073	81975.128616	59.239092
2358.890469	81794.898749	59.244097
2358.753724	81606.696537	59.249101
2358.289807	81418.528869	59.254106
2357.306571	81221.496299	59.259111
2356.847009	81037.989628	59.264116
2355.756910	80861.625662	59.269121
2355.467360	80665.559446	59.274125
2354.712586	80471.191236	59.279130
2354.184004	80277.270636	59.284135
2353.696630	80085.297240	59.289140
2352.892252	79899.225256	59.294145
2352.343925	79702.733854	59.299149
2351.350283	79510.922086	59.304154
2350.514015	79314.441996	59.309159
2350.216981	79133.492964	59.314164
2349.402217	78939.446492	59.319169
2349.139147	78743.292883	59.324173
2348.176200	78551.897074	59.329178
2347.266446	78351.794070	59.334183
2346.862925	78161.574250	59.339188
2345.953170	77982.741243	59.344193
2345.505542	77781.233482	59.349197
2344.804479	77596.217820	59.354202
2344.094587	77397.087304	59.359207
2343.417502	77222.007002	59.364212
2342.624596	77029.920443	59.369217
2342.234807	76830.174424	59.374221
2341.473887	76647.762101	59.379226
2340.735020	76456.318690	59.384231
2340.084072	76262.917917	59.389236
2339.604121	76074.801593	59.394241
2339.046529	75881.833180	59.399245
2338.179663	75693.737374	59.404250
2337.343527	75487.213359	59.409255
2337.211267	75305.410391	59.414260
2336.046648	75117.880352	59.419265
2335.467449	74913.931841	59.424269
2334.848723	74726.756063	59.429274
2334.142048	74547.851382	59.434279
2333.809974	74349.457490	59.439284
2333.009587	74168.188839	59.444289
2332.479084	73964.229549	59.449293
2331.390607	73774.520531	59.454298
2331.153140	73580.281626	59.459303
2330.705265	73388.003901	59.464308
2329.287196	73199.011459	59.469313
2328.986352	73002.070374	59.474317
2328.383778	72818.603253	59.479322
2327.568188	72624.186534	59.484327
2327.207540	72430.377432	59.489332
2326.338962	72240.020944	59.494337
2325.635178	72040.574896	59.499341
2325.041760	71843.888012	59.504346
2324.301152	71656.506868	59.509351
2324.070854	71450.188119	59.514356
2322.727922	71277.456905	59.519361
2322.108977	71078.855912	59.524365
2321.692130	70886.496064	59.529370
2320.894857	70696.896887	59.534375
2320.288091	70499.230952	59.539380
2319.467881	70315.656768	59.544385
2319.092809	70122.505942	59.549389
2318.262233	69935.282057	59.554394
2317.546730	69752.424958	59.559399
2317.121759	69557.406337	59.564404
2316.035972	69364.476976	59.569409
2315.770402	69174.770153	59.574413
2315.061160	68979.954353	59.579418
2314.326786	68794.480592	59.584423
2313.627912	68604.588298	59.589428
2312.992606	68412.116270	59.594433
2312.517774	68219.570027	59.599437
2311.732502	68033.136175	59.604442
2311.258955	67836.153644	59.609447
2310.549233	67645.233701	59.614452
2309.353965	67455.203293	59.619457
2308.858714	67257.381381	59.624461
2308.723804	67082.804589	59.629466
2307.872741	66879.881288	59.634471
2307.396568	66690.029357	59.639476
2306.535193	66494.622882	59.644481
2305.872686	66299.069689	59.649485
2305.436945	66112.326544	59.654490
2304.678851	65914.784837	59.659495
2304.358478	65716.947768	59.664500
2303.388510	65523.043899	59.669505
2302.602061	65322.251367	59.674509
2302.033324	65127.736918	59.679514
2301.175538	64928.207348	59.684519
2300.560410	64732.770194	59.689524
2299.711179	64540.915168	59.694529
2299.428449	64341.050397	59.699533
2298.510128	64150.802834	59.704538
2297.975067	63959.654203	59.709543
2297.351607	63756.252826	59.714548
2296.644764	63568.611731	59.719553
2296.093416	63370.917797	59.724557
2295.436171	63176.864621	59.729562
2294.573633	62982.741495	59.734567
2294.065282	62777.394733	59.739572
2293.126336	62595.976787	59.744577
2292.497665	62393.018196	59.749581
2291.847162	62215.648473	59.754586
2291.154626	62035.124418	59.759591
2290.818975	61827.398852	59.764596
2289.921892	61641.943860	59.769601
2289.464195	61443.596673	59.774605
2288.722695	61243.577597	59.779610
2287.995169	61061.124661	59.784615
2287.337503	60862.789960	59.789620
2286.657223	60674.986532	59.794625
2286.300827	60473.107022	59.799629
2285.568331	60276.971433	59.804634
2284.977229	60085.253497	59.809639
2284.333663	59883.701254	59.814644
2283.408259	59681.268395	59.819649
2282.808421	59482.815650	59.824653
2281.962627	59287.841589	59.829658
2281.643040	59097.059320	59.834663
2280.656510	58907.942075	59.839668
2279.844692	58710.863731	59.844673
2279.321153	58510.529056	59.849677
2278.853724	58326.380780	59.854682
2277.913014	58143.461489	59.859687
2277.372834	57941.496024	59.864692
2276.583116	57757.819115	59.869697
2276.001124	57563.622052	59.874701
2275.592806	57369.266555	59.879706
2274.835297	57171.164134	59.884711
2274.249947	56974.574710	59.889716
2273.414459	56781.578095	59.894721
2273.040332	56580.408199	59.899725
2272.462770	56395.771198	59.904730
2271.391378	56200.438087	59.909735
2270.948222	56000.807746	59.914740
2270.016357	55809.586724	59.919745
2269.574731	55610.770553	59.924750
2268.702013	55423.019052	59.929754
2268.034104	55221.654251	59.934759
2267.680052	55032.574463	59.939764
2266.793741	54838.584121	59.944769
2266.448383	54639.462579	59.949774
2265.567849	54451.725440	59.954778
2264.802093	54260.608170	59.959783
2264.592681	54061.635921	59.964788
2263.667253	53864.494499	59.969793
2263.010871	53668.198581	59.974798
2262.614345	53469.177032	59.979802
2261.811505	53267.450138	59.984807
2261.122546	53073.064405	59.989812
2260.162045	52881.641260	59.994817
2259.652855	52675.963353	59.999822
2258.783231	52486.770239	60.004826
2258.050007	52290.779850	60.009831
2257.975672	52102.648038	60.014836
2257.039806	51907.041996	60.019841
2256.440288	51711.467005	60.024846
2255.429242	51518.620332	60.029850
2254.752336	51319.151140	60.034855
2254.313962	51128.005493	60.039860
2253.751646	50936.043091	60.044865
2253.438600	50729.884834	60.049870
2252.620693	50530.484715	60.054874
2251.712876	50339.915453	60.059879
2251.477066	50136.652980	60.064884
2250.581227	49945.437441	60.069889
2249.564088	49737.551454	60.074894
2248.869045	49552.505981	60.079898
2248.594818	49358.752627	60.084903
2247.845665	49157.654870	60.089908
2247.105851	48966.146680	60.094913
2246.428031	48761.900652	60.099918
2246.218400	48570.831460	60.104922
2245.214686	48371.393172	60.109927
2244.683653	48169.579194	60.114932
2244.026208	47972.580096	60.119937
2243.418201	47773.123745	60.124942
2242.537260	47570.052956	60.129946
2241.989862	47374.947373	60.134951
2241.469860	47168.935872	60.139956
2240.368026	46980.223762	60.144961
2240.162532	46775.416447	60.149966
2239.305262	46583.357953	60.154970
2238.229971	46385.683648	60.159975
2237.757603	46177.468323	60.164980
2236.916351	45998.635316	60.169985
2236.316066	45794.411265	60.174990
2235.762777	45605.161953	60.179994
2234.815371	45410.473674	60.184999
2234.500530	45209.013531	60.190004
2233.741535	45027.976000	60.195009
2232.867814	44829.698969	60.200014
2232.334085	44628.324501	60.205018
2231.780847	44440.903209	60.210023
2231.403129	44245.435427	60.215028
2230.264205	44057.497566	60.220033
2230.081247	43857.926537	60.225038
2229.206981	43664.267664	60.230042
2228.724961	43478.863177	60.235047
2228.008625	43275.714814	60.240052
2227.117986	43080.037857	60.245057
2226.716101	42883.128135	60.250062
2226.081458	42691.092931	60.255066
2225.041810	42494.557572	60.260071
2224.651289	42299.173803	60.265076
2223.748442	42102.681288	60.270081
2223.445287	41904.805691	60.275086
2222.685760	41715.953936	60.280090
2221.889115	41522.161250	60.285095
2221.714389	41311.398673	60.290100
2220.965409	41115.952338	60.295105
2220.558973	40915.362894	60.300110
2219.679659	40711.989103	60.305114
2218.854983	40519.495967	60.310119
2218.365513	40302.999645	60.315124
2217.319375	40112.664741	60.320129
2217.117885	39911.254559	60.325134
2216.190197	39716.910175	60.330138
2215.489500	39508.303646	60.335143
2214.989722	39302.458107	60.340148
2214.184301	39117.057013	60.345153
2213.825693	38907.728535	60.350158
2213.259346	38710.358370	60.355162
2212.220391	38501.722953	60.360167
2211.629570	38309.606530	60.365172
2211.032473	38103.281899	60.370177
2210.550580	37895.969328	60.375182
2209.696390	37697.109004	60.380186
2208.630611	37499.825793	60.385191
2208.548783	37285.083093	60.390196
2207.575491	37097.517669	60.395201
2207.082957	36897.615125	60.400206
2206.234214	36701.155646	60.405210
2205.831435	36495.124876	60.410215
2205.078560	36293.268102	60.415220
2204.151342	36097.744869	60.420225
2203.404542	35886.700764	60.425230
2202.775304	35697.310297	60.430234
2202.148859	35495.577397	60.435239
2201.598914	35295.930579	60.440244
2200.924783	35101.535759	60.445249
2200.309813	34888.054053	60.450254
2199.456916	34702.340698	60.455258
2199.102496	34506.109827	60.460263
2198.301996	34303.448491	60.465268
2197.504162	34105.495689	60.470273
2197.170074	33905.937116	60.475278
2196.456765	33709.772526	60.480282
2195.545421	33512.783516	60.485287
2194.970228	33304.628948	60.490292
2194.308693	33108.695545	60.495297
2193.648763	32912.209511	60.500302
2192.628688	32725.816186	60.505306
2192.033145	32522.303328	60.510311
2191.744775	32314.055643	60.515316
2190.869269	32127.745677	60.520321
2190.189925	31931.370749	60.525326
2189.609445	31738.763886	60.530330
2188.786238	31535.661139	60.535335
2188.141979	31337.955614	60.540340
2187.655594	31150.109619	60.545345
2186.957312	30953.123603	60.550350
2186.172868	30755.611635	60.555354
2185.532690	30553.621744	60.560359
2184.940568	30361.841830	60.565364
2184.255917	30172.317758	60.570369
2183.686190	29969.712399	60.575374
2182.876373	29775.104544	60.580378
2181.815161	29585.654881	60.585383
2181.587335	29384.347109	60.590388
2180.740265	29186.287292	60.595393
2180.411468	28994.412110	60.600398
2179.367877	28808.261248	60.605402
2178.596387	28613.678527	60.610407
2177.997526	28412.196705	60.615412
2177.288360	28228.678897	60.620417
2176.704651	28036.084456	60.625422
2175.945209	27843.872469	60.630426
2175.505244	27651.319822	60.635431
2175.053876	27459.820244	60.640436
2174.325290	27271.430061	60.645441
2173.659020	27070.389472	60.650446
2172.887708	26875.601642	60.655450
2171.879912	26686.501122	60.660455
2171.833546	26486.782514	60.665460
2170.922222	26303.187455	60.670465
2170.160426	26102.125091	60.675470
2169.557577	25916.749468	60.680474
2168.849336	25719.434223	60.685479
2168.284564	25527.553772	60.690484
2167.611174	25339.858969	60.695489
2167.111655	25139.615259	60.700494
2166.365374	24953.155953	60.705498
2165.681729	24748.563894	60.710503
2165.475403	24549.077124	60.715508
2164.444976	24371.281085	60.720513
2163.922389	24170.441874	60.725518
2163.112102	23970.534515	60.730522
2162.620839	23776.539006	60.735527
2162.076711	23576.524866	60.740532
2161.005252	23379.818815	60.745537
2160.501477	23191.691914	60.750542
2159.908749	22995.435866	60.755546
2159.017846	22789.790694	60.760551
2158.726352	22591.442675	60.765556
2157.811222	22403.174766	60.770561
2157.062884	22201.211708	60.775566
2156.820082	22001.487001	60.780570
2155.830445	21819.423748	60.785575
2155.048885	21611.655594	60.790580
2154.533557	21422.982170	60.795585
2153.993124	21220.557255	60.800590
2153.093247	21029.833432	60.805594
2152.507859	20839.372330	60.810599
2152.135652	20635.426477	60.815604
2151.032407	20447.716994	60.820609
2150.533467	20249.222000	60.825614
2149.893132	20049.059192	60.830618
2149.002071	19858.757516	60.835623
2148.255903	19660.466279	60.840628
2147.485750	19477.308896	60.845633
2146.943220	19280.614943	60.850638
2146.369347	19097.720206	60.855642
2145.631959	18900.506138	60.860647
2145.456203	18706.574481	60.865652
2144.153613	18518.375762	60.870657
2143.712367	18337.971420	60.875662
2143.052483	18144.406543	60.880666
2142.361020	17938.170205	60.885671
2141.874612	17748.208530	60.890676
2140.854036	17565.805574	60.895681
2140.181301	17376.764482	60.900686
2139.305424	17191.033052	60.905690
2138.883606	17004.935015	60.910695
2138.583444	16811.088301	60.915700
2137.610878	16626.497091	60.920705
2137.135727	16446.968988	60.925710
2136.310932	16254.381664	60.930714
2135.589954	16063.608539	60.935719
2135.011694	15875.604171	60.940724
2134.102831	15701.231766	60.945729
2133.614668	15497.145677	60.950734
2132.771511	15321.190326	60.955738
2132.002896	15140.239886	60.960743
2131.701878	14948.351848	60.965748
2130.756469	14771.992781	60.970753
2130.212828	14585.232549	60.975758
2129.421404	14400.811955	60.980762
2128.350792	14214.537988	60.985767
2127.936171	14041.939643	60.990772
2126.821550	13869.336117	60.995777
2126.248798	13673.684542	61.000782
2125.739104	13504.775236	61.005786
2125.047550	13336.909559	61.010791
2124.350699	13158.359622	61.015796
2123.568512	13001.806777	61.020801
2122.757966	12821.477955	61.025806
2121.977274	12639.594567	61.030810
2121.426109	12484.267791	61.035815
2121.113390	12307.667062	61.040820
2119.999333	12145.541150	61.045825
2119.705379	11972.332783	61.050830
2118.847401	11807.143405	61.055834
2118.001442	11636.853785	61.060839
2117.335643	11469.965095	61.065844
2116.777945	11302.115969	61.070849
2115.637567	11141.880777	61.075854
2114.787381	10986.141906	61.080858
2113.930189	10826.679832	61.085863
2113.509597	10673.201373	61.090868
2112.213887	10538.138617	61.095873
2111.800933	10379.959639	61.100878
2110.537214	10244.487491	61.105882
2109.602561	10105.747338	61.110887
2109.011951	9970.359249	61.115892
2108.148722	9839.446661	61.120897
2107.224650	9720.884766	61.125902
2106.257787	9592.936873	61.130906
2105.077299	9474.912288	61.135911
2104.765523	9357.470368	61.140916
2103.944446	9246.947780	61.145921
2103.321482	9127.564075	61.150926
2102.596311	9029.557836	61.155930
2101.866783	8917.575009	61.160935
2101.212129	8816.282445	61.165940
2100.269318	8711.221732	61.170945
2099.801537	8594.393546	61.175950
2099.227274	8495.441033	61.180954
2098.421187	8388.458775	61.185959
2097.700870	8282.519250	61.190964
2096.655083	8196.923430	61.195969
2096.318667	8088.161196	61.200974
2095.670489	7982.716461	61.205978
2094.972374	7894.932435	61.210983
2094.335071	7799.840804	61.215988
2093.526771	7701.252534	61.220993
2092.886741	7600.325208	61.225998
2091.818621	7513.700247	61.231002
2090.956194	7427.914078	61.236007
2090.739822	7337.505675	61.241012
2089.786522	7258.437151	61.246017
2089.502434	7155.870736	61.251022
2088.599685	7068.832427	61.256026
2087.815501	6994.259812	61.261031
2087.208721	6895.389307	61.266036
2086.454269	6818.816673	61.271041
2085.658014	6739.476714	61.276046
2084.847652	6656.570724	61.281050
2084.213045	6577.432381	61.286055
2083.839476	6491.342132	61.291060
2082.909655	6422.305839	61.296065
2082.399990	6340.980457	61.301070
2081.721785	6266.798157	61.306074
2080.812147	6195.271795	61.311079
2079.855597	6114.379826	61.316084
2079.327016	6048.637201	61.321089
2078.686682	5976.970567	61.326094
2077.948515	5912.596444	61.331098
2077.059428	5841.153721	61.336103
2076.999203	5765.532571	61.341108
2075.912922	5707.249588	61.346113
2075.504969	5635.251945	61.351118
2074.979332	5563.203908	61.356122
2074.241016	5498.463249	61.361127
2073.329451	5424.322972	61.366132
2072.592533	5356.855143	61.371137
2071.560719	5285.323374	61.376142
2071.138376	5232.033130	61.381146
2070.471091	5169.460408	61.386151
2070.143997	5102.196111	61.391156
2069.273874	5045.753944	61.396161
2068.933054	4980.582565	61.401166
2068.303467	4915.163873	61.406170
2067.807935	4857.415206	61.411175
2066.955320	4787.566617	61.416180
2065.973150	4723.822409	61.421185
2065.408121	4656.644422	61.426190
2064.255998	4597.867536	61.431194
2063.702823	4540.802036	61.436199
2063.530046	4477.338252	61.441204
2062.761183	4427.176374	61.446209
2062.056760	4359.827829	61.451214
2061.450855	4302.228983	61.456218
2060.883049	4250.512809	61.461223
2060.298517	4173.633493	61.466228
2059.265431	4123.506683	61.471233
2058.859093	4058.499621	61.476238
2057.894967	4003.052771	61.481242
2057.281730	3946.615072	61.486247
2056.806897	3885.005496	61.491252
2056.053585	3830.671024	61.496257
2055.538529	3780.751855	61.501262
2055.020192	3717.724732	61.506266
2054.270510	3659.778166	61.511271
2053.459224	3599.150651	61.516276
2052.825550	3546.274647	61.521281
2052.123698	3480.100107	61.526286
2051.515175	3424.667636	61.531290
2050.733687	3372.542069	61.536295
2050.094333	3311.457066	61.541300
2049.443583	3265.771030	61.546305
2048.725139	3201.071222	61.551310
2048.028310	3151.015051	61.556314
2047.348921	3101.973636	61.561319
2046.805653	3044.971516	61.566324
2046.095347	2998.515006	61.571329
2045.595165	2934.224963	61.576334
2045.405627	2885.599451	61.581338
2044.096292	2830.228369	61.586343
2043.817652	2763.228099	61.591348
2042.831235	2723.015677	61.596353
2042.341745	2673.720809	61.601358
2041.762781	2606.615123	61.606362
2041.039162	2546.702794	61.611367
2040.510646	2487.340963	61.616372
2039.203378	2448.236948	61.621377
2038.884422	2384.979666	61.626382
2037.949386	2337.425317	61.631386
2037.544166	2288.910135	61.636391
2036.875264	2230.297924	61.641396
2036.221315	2185.193813	61.646401
2035.559288	2124.279812	61.651406
2035.035716	2081.152844	61.656410
2034.164738	2026.982527	61.661415
2033.942090	1964.958539	61.666420
2032.646117	1920.682611	61.671425
2032.586870	1868.570040	61.676430
2031.941809	1815.643739	61.681434
2031.189254	1772.225179	61.686439
2030.583654	1707.524325	61.691444
2029.335592	1655.543573	61.696449
2028.821011	1617.533571	61.701454
2028.119672	1560.753940	61.706458
2027.789508	1508.911166	61.711463
2027.038794	1458.375705	61.716468
2026.190621	1432.074006	61.721473
2025.596736	1373.348459	61.726478
2025.112080	1318.696026	61.731482
2024.141381	1270.463205	61.736487
2023.555279	1221.154663	61.741492
2022.904681	1172.944711	61.746497
2022.275442	1121.676727	61.751502
2021.706366	1077.754850	61.756506
2021.009230	1030.249822	61.761511
2020.462929	969.907376	61.766516
2019.594242	936.722800	61.771521
2018.963396	881.680438	61.776526
2018.319035	838.392590	61.781530
2017.287123	792.591051	61.786535
2016.694443	737.710346	61.791540
2015.971913	701.293848	61.796545
2015.326919	654.622334	61.801550
2015.044459	629.667427	61.806554
2014.328948	582.628848	61.811559
2013.787575	539.172581	61.816564
2012.594776	498.445531	61.821569
2012.229292	455.922004	61.826574
2011.559939	405.667466	61.831578
2010.531100	368.378652	61.836583
2010.428032	327.204775	61.841588
2009.674514	284.183490	61.846593
2008.904058	241.896741	61.851598
2008.152719	198.701896	61.856602
2007.194953	162.226309	61.861607
2006.542946	127.492159	61.866612
2005.645727	107.130068	61.871617
2004.924317	65.988817	61.876622
2004.148990	32.993354	61.881626
2002.976812	14.755036	61.886631
2001.894577	8.602467	61.891636
1998.356343	54.306875	61.896641
1997.838910	64.428819	61.901646
1997.922122	56.416563	61.906650
1998.065971	58.749031	61.911655
1997.783756	57.162541	61.916660
1997.709056	59.662153	61.921665
1997.400517	58.694856	61.926670
1996.827566	57.577127	61.931674
1995.190502	70.658502	61.936679
1994.530343	65.189572	61.941684
1993.168722	77.317338	61.946689
1992.144867	69.453937	61.951694
1992.009921	68.503250	61.956698
1991.813812	79.821596	61.961703
1991.989385	65.242388	61.966708
1991.132055	77.447830	61.971713
1990.176792	74.126244	61.976718
1989.694824	67.329620	61.981722
1988.681035	74.169823	61.986727
1988.031056	73.266169	61.991732
1987.490373	70.681473	61.996737
1987.364416	78.554057	62.001742
1986.778198	77.654478	62.006746
1985.844130	82.151280	62.011751
1985.339910	71.696471	62.016756
1984.320402	79.146294	62.021761
1983.764956	76.513478	62.026766
1982.578778	76.623744	62.031770
1982.018802	83.981726	62.036775
1981.037793	76.136759	62.041780
1981.247639	78.162286	62.046785
1980.563654	76.483432	62.051790
1980.396880	71.421916	62.056794
1978.987013	83.311342	62.061799
1978.590024	81.804567	62.066804
1977.588805	82.180377	62.071809
1976.797582	77.861354	62.076814
1976.134530	75.034302	62.081818
1975.251409	82.211749	62.086823
1975.516592	72.670915	62.091828
1975.184803	75.219210	62.096833
1974.155781	74.755758	62.101838
1973.183285	76.527357	62.106842
1972.746870	84.927030	62.111847
1971.589912	72.685024	62.116852
1971.253255	88.229868	62.121857
1970.714973	78.985266	62.126862
1970.276083	76.813354	62.131866
1969.120473	89.354729	62.136871
1968.873021	81.295585	62.141876
1968.030651	81.012251	62.146881
1967.375032	78.199791	62.151886
1967.101759	84.965072	62.156890
1965.967168	88.754106	62.161895
1965.325301	78.207600	62.166900
1964.381000	90.939373	62.171905
1963.923285	86.162146	62.176910
1963.510633	79.163711	62.181914
1962.501980	90.338192	62.186919
1962.064981	84.091100	62.191924
1961.236581	87.002061	62.196929
1960.479019	85.407428	62.201934
1960.495243	89.750282	62.206938
1959.732088	92.273996	62.211943
1958.922875	88.564962	62.216948
1958.158183	93.429139	62.221953
1957.491282	91.578843	62.226958
1957.175229	92.155015	62.231962
1956.536026	100.063326	62.236967
1955.606820	85.648384	62.241972
1954.894436	86.680116	62.246977
1954.162205	85.387397	62.251982
1953.732723	92.090737	62.256986
1952.751701	94.527601	62.261991
1952.585172	91.635949	62.266996
1951.525430	91.230997	62.272001
1950.820803	93.623998	62.277006
1950.393849	87.167154	62.282010
1950.044807	89.771810	62.287015
1949.235113	80.644402	62.292020
1948.427948	98.222515	62.297025
1948.058465	99.406415	62.302030
1947.487022	89.446402	62.307034
1945.876699	92.762158	62.312039
1945.735279	87.975740	62.317044
1945.170327	97.479197	62.322049
1944.368443	91.513942	62.327054
1943.423001	91.850951	62.332058
1943.122445	100.768397	62.337063
1942.751562	82.909073	62.342068
1941.357764	95.928235	62.347073
1941.138780	82.815131	62.352078
1940.684759	88.128327	62.357082
1939.803398	97.950083	62.362087
1938.998463	87.929357	62.367092
1938.066524	95.896742	62.372097
1937.679466	90.105355	62.377102
1937.411042	92.722450	62.382106
1936.198280	95.060478	62.387111
1935.939517	83.666273	62.392116
1935.325358	91.151135	62.397121
1934.442067	92.731972	62.402126
1934.411978	91.856110	62.407130
1933.431925	92.398890	62.412135
1933.155427	86.079023	62.417140
1932.657587	89.290772	62.422145
1931.201251	88.185517	62.427150
1930.460522	86.244442	62.432154
1929.210848	97.250606	62.437159
1929.273067	92.950692	62.442164
1928.529816	91.730692	62.447169
1928.421945	84.732777	62.452174
1927.732327	89.474657	62.457178
1926.809656	87.248643	62.462183
1926.649785	84.281821	62.467188
1925.453796	93.738769	62.472193
1924.695206	91.493022	62.477198
1923.784985	79.153531	62.482202
1922.752704	90.413775	62.487207
1923.212745	76.415471	62.492212
1922.173230	90.543784	62.497217
1920.898525	91.615884	62.502222
1920.781034	79.890179	62.507226
1919.707037	87.733452	62.512231
1919.697186	78.001297	62.517236
1919.166946	81.782742	62.522241
1918.302555	91.008866	62.527246
1917.898777	74.499933	62.532250
1917.191159	83.541898	62.537255
1916.159218	84.390966	62.542260
1915.046918	87.403768	62.547265
1914.566463	87.417829	62.552270
1913.996528	81.605013	62.557274
1913.157719	81.393671	62.562279
1912.999600	83.892334	62.567284
1912.179824	90.980898	62.572289
1911.715787	86.690392	62.577294
1911.342768	84.651540	62.582298
1910.610432	92.573058	62.587303
1910.057660	88.810726	62.592308
1908.623397	90.113160	62.597313
1907.445844	88.679818	62.602318
1907.862466	83.710220	62.607322
1907.024543	94.045484	62.612327
1906.285565	85.901933	62.617332
1905.525402	86.815104	62.622337
1905.366873	88.079069	62.627342
1904.897486	85.699118	62.632346
1903.554057	82.748257	62.637351
1902.839911	81.856385	62.642356
1901.598645	85.466830	62.647361
1901.736389	89.424537	62.652366
1901.279684	77.812601	62.657370
1900.456387	86.598538	62.662375
1899.877489	80.747724	62.667380
1899.290772	87.370366	62.672385
1898.662266	90.044614	62.677390
1898.181923	82.495535	62.682394
1896.802189	89.180964	62.687399
1896.268273	86.825450	62.692404
1895.510776	85.025820	62.697409
1894.921119	83.672641	62.702414
1894.406509	83.841938	62.707418
1893.852144	88.814673	62.712423
1893.865659	75.448640	62.717428
1892.694949	85.007237	62.722433
1891.590417	90.226567	62.727438
1890.920830	81.078523	62.732442
1889.711099	86.268817	62.737447
1889.562146	77.408728	62.742452
1888.764142	81.606417	62.747457
1888.291887	87.389295	62.752462
1888.353737	82.375079	62.757466
1887.565993	92.211946	62.762471
1887.456670	85.592738	62.767476
1886.024694	90.622766	62.772481
1885.167704	87.063268	62.777486
1884.683625	84.622575	62.782490
1883.491731	91.514742	62.787495
1883.424634	85.691507	62.792500
1882.748838	90.991026	62.797505
1882.118249	89.455110	62.802510
1881.179099	87.105571	62.807514
1879.887657	97.896030	62.812519
1879.506885	88.421444	62.817524
1878.972070	93.753781	62.822529
1878.758137	86.835784	62.827534
1878.561078	82.999654	62.832538
1877.793299	84.464402	62.837543
1877.336825	81.959405	62.842548
1875.732509	88.571679	62.847553
1875.021691	87.203042	62.852558
1874.543555	82.036414	62.857562
1874.031797	97.299971	62.862567
1873.709745	79.838203	62.867572
1872.960092	88.129908	62.872577
1872.132667	83.487079	62.877582
1871.288804	93.170430	62.882586
1870.580042	98.062021	62.887591
1870.226218	84.536668	62.892596
1869.629341	83.071100	62.897601
1868.800960	85.508994	62.902606
1868.305586	84.074624	62.907610
1866.880875	89.593944	62.912615
1866.633117	84.758182	62.917620
1865.840071	81.634824	62.922625
1865.277341	83.257840	62.927630
1865.209444	90.490424	62.932634
1864.526775	86.404944	62.937639
1863.852656	83.070319	62.942644
1862.676687	87.889410	62.947649
1862.122628	93.827204	62.952654
1861.808807	85.731303	62.957658
1860.904400	84.494325	62.962663
1860.483094	84.205692	62.967668
1859.217097	88.480829	62.972673
1858.675711	85.823732	62.977678
1858.218140	78.846643	62.982682
1857.489545	85.863974	62.987687
1857.306581	86.245565	62.992692
1856.787050	91.583364	62.997697
1855.147337	86.791930	63.002702
1854.813763	84.363624	63.007706
1853.951140	89.621839	63.012711
1853.898525	81.803027	63.017716
1853.138287	87.606389	63.022721
1852.486129	83.457722	63.027726
1851.655685	87.925502	63.032730
1850.607797	92.478262	63.037735
1850.308908	71.135080	63.042740
1849.299821	84.159431	63.047745
1848.983990	90.359035	63.052750
1848.771919	84.423197	63.057754
1847.935653	87.783296	63.062759
1846.860853	78.360543	63.067764
1846.085501	89.687257	63.072769
1845.524245	87.325055	63.077774
1845.257316	76.723808	63.082778
1844.430237	79.893212	63.087783
1844.022137	75.234297	63.092788
1842.876901	79.807240	63.097793
1842.020427	84.574045	63.102798
1841.497680	82.415468	63.107802
1840.934386	90.639751	63.112807
1840.560860	87.154914	63.117812
1840.245626	90.610506	63.122817
1839.178283	90.522197	63.127822
1838.017129	88.141682	63.132826
1837.225663	90.335605	63.137831
1837.100817	77.407860	63.142836
1836.559100	84.095907	63.147841
1835.942106	84.682016	63.152846
1835.698227	85.256206	63.157850
1834.651950	97.505880	63.162855
1833.681124	85.720100	63.167860
1833.110324	84.818108	63.172865
1832.637166	91.619855	63.177870
1832.081731	83.007224	63.182874
1831.025968	90.369813	63.187879
1830.242153	81.028609	63.192884
1829.541622	78.111353	63.197889
1829.196842	84.657751	63.202894
1828.663552	86.093174	63.207898
1827.966020	89.849151	63.212903
1827.806662	80.667444	63.217908
1826.602555	84.986386	63.222913
1825.811325	91.896973	63.227918
1825.477283	82.810804	63.232922
1824.513897	92.841146	63.237927
1823.345274	82.036106	63.242932
1822.705735	93.211956	63.247937
1822.642214	82.635190	63.252942
1822.088364	82.886424	63.257946
1821.488993	87.990894	63.262951
1821.020724	81.218940	63.267956
1820.158569	86.073386	63.272961
1819.032160	84.819625	63.277966
1818.542270	83.426972	63.282970
1818.116618	85.553366	63.287975
1817.528148	81.637452	63.292980
1816.869592	96.142139	63.297985
1815.445650	80.102690	63.302990
1814.939653	88.816199	63.307994
1814.050001	88.079946	63.312999
1813.645402	81.359388	63.318004
1813.350577	85.727957	63.323009
1813.037270	94.443996	63.328014
1812.881209	87.139928	63.333018
1811.444062	85.566490	63.338023
1810.792266	74.930154	63.343028
1809.752577	87.431094	63.348033
1809.245494	89.726536	63.353038
1809.160939	84.885374	63.358042
1808.550994	85.552373	63.363047
1807.174660	82.160506	63.368052
1806.510755	85.545294	63.373057
1806.156245	72.680827	63.378062
1805.853972	81.508649	63.383066
1804.803684	87.712884	63.388071
1804.136169	79.777227	63.393076
1803.191941	85.272338	63.398081
1802.599604	79.215527	63.403086
1802.099785	76.767889	63.408090
1801.823065	89.841574	63.413095
1800.967929	74.899296	63.418100
1799.764438	82.983937	63.423105
1798.960778	79.073805	63.428110
1798.794845	81.770831	63.433114
1798.275620	90.696179	63.438119
1798.216687	75.053487	63.443124
1796.864785	86.455966	63.448129
1795.859045	81.280075	63.453134
1795.294122	88.504826	63.458138
1794.594941	95.004991	63.463143
1794.566840	81.819039	63.468148
1793.832869	85.020986	63.473153
1792.992593	83.736004	63.478158
1792.094019	82.408238	63.483162
1791.215801	87.591674	63.488167
1790.956961	83.561934	63.493172
1790.392801	87.793489	63.498177
1789.764895	80.316753	63.503182
1788.998824	86.756571	63.508186
1788.023164	90.236589	63.513191
1787.796018	76.159719	63.518196
1786.931271	80.886851	63.523201
1786.570210	84.870118	63.528206
1785.219344	75.574805	63.533210
1784.344010	82.675370	63.538215
1784.200737	82.181758	63.543220
1783.467935	78.090070	63.548225
1783.171398	83.898678	63.553230
1782.815967	84.965248	63.558234
1781.867990	88.262676	63.563239
1781.011023	86.234444	63.568244
1780.372840	86.301955	63.573249
1779.636085	93.208636	63.578254
1779.640252	81.547218	63.583258
1778.142802	90.321941	63.588263
1777.415833	81.796485	63.593268
1777.121122	85.479059	63.598273
1776.357893	79.624428	63.603278
1776.092986	82.338746	63.608282
1775.095077	88.545714	63.613287
1774.284547	85.297427	63.618292
1773.346088	84.215698	63.623297
1773.079827	88.366845	63.628302
1772.672296	81.910114	63.633306
1772.121802	93.546498	63.638311
1771.401156	77.354425	63.643316
1770.544542	77.999092	63.648321
1770.097543	79.078624	63.653326
1769.824507	75.458000	63.658330
1768.339574	91.558883	63.663335
1767.718187	79.331306	63.668340
1767.171643	80.033979	63.673345
1766.688849	79.980629	63.678350
1765.713239	79.880940	63.683354
1764.507393	86.379546	63.688359
1764.151123	84.431099	63.693364
1763.480267	82.467943	63.698369
1762.914649	80.358768	63.703374
1762.790762	84.749086	63.708378
1762.205172	93.615590	63.713383
1761.626376	78.500142	63.718388
1760.660125	82.317720	63.723393
1759.876055	85.150736	63.728398
1759.783698	84.084489	63.733402
1758.565307	87.265584	63.738407
1757.667470	85.149231	63.743412
1756.945712	90.041330	63.748417
1756.286246	88.295564	63.753422
1755.981801	83.145541	63.758426
1755.361788	90.697592	63.763431
1755.037469	88.285177	63.768436
1753.821066	86.648338	63.773441
1753.182631	96.612916	63.778446
1753.053213	83.884604	63.783450
1752.099281	87.168794	63.788455
1751.154053	87.851191	63.793460
1750.281427	83.694980	63.798465
1749.745993	87.576626	63.803470
1749.577814	79.448166	63.808474
1748.731148	85.128078	63.813479
1748.116046	82.796526	63.818484
1747.205781	90.276389	63.823489
1746.601456	85.314330	63.828494
1746.536743	73.487240	63.833498
1745.540206	81.035990	63.838503
1744.878500	84.007278	63.843508
1743.685583	91.092048	63.848513
1743.017120	75.069901	63.853518
1742.891773	75.475468	63.858522
1742.060750	81.156049	63.863527
1742.019225	75.262539	63.868532
1740.913682	78.788423	63.873537
1740.231221	81.507539	63.878542
1739.545772	74.449968	63.883546
1738.836172	87.190253	63.888551
1737.912367	82.922324	63.893556
1737.553374	77.110758	63.898561
1737.058202	84.764413	63.903566
1736.628572	83.950415	63.908570
1735.252438	79.440492	63.913575
1734.721809	71.147236	63.918580
1734.045190	81.236140	63.923585
1733.797821	82.380176	63.928590
1732.839386	79.614285	63.933594
1732.062569	87.241697	63.938599
1731.692212	78.763717	63.943604
1731.189432	78.688314	63.948609
1730.365840	93.121438	63.953614
1729.536931	91.353698	63.958618
1728.498810	86.810607	63.963623
1728.170843	76.953941	63.968628
1727.927063	82.628017	63.973633
1726.887073	93.377026	63.978638
1725.832524	85.759891	63.983642
1725.349607	89.836631	63.988647
1725.053816	87.228879	63.993652
1724.520938	89.244577	63.998657
1723.870751	92.950483	64.003662
1722.909130	83.915098	64.008666
1721.691819	85.935393	64.013671
1721.329836	80.362426	64.018676
1720.932365	81.282714	64.023681
1720.557432	79.781941	64.028686
1719.997126	81.078169	64.033690
1718.739490	79.537782	64.038695
1718.058049	78.383723	64.043700
1717.548010	92.489516	64.048705
1717.053078	96.773173	64.053710
1716.868708	82.132854	64.058714
1715.591526	89.719872	64.063719
1715.135895	82.365615	64.068724
1714.416545	84.556005	64.073729
1713.878275	86.714488	64.078734
1712.933495	85.234812	64.083738
1711.943333	87.211159	64.088743
1711.815601	82.561367	64.093748
1711.412981	95.054221	64.098753
1710.752914	87.070100	64.103758
1709.729611	91.385614	64.108762
1708.881295	98.054558	64.113767
1708.149370	83.267795	64.118772
1707.599383	87.042948	64.123777
1707.268045	89.207999	64.128782
1706.464840	81.043183	64.133786
1705.393507	83.535471	64.138791
1705.160333	80.662312	64.143796
1704.484730	80.090806	64.148801
1703.962957	90.899459	64.153806
1703.325525	79.773597	64.158810
1702.286573	89.219875	64.163815
1701.878823	88.998501	64.168820
1701.470001	80.452517	64.173825
1700.867654	83.982094	64.178830
1699.870381	88.151551	64.183834
1698.902263	90.450833	64.188839
1698.792069	80.394010	64.193844
1697.901701	86.189685	64.198849
1696.771437	90.369222	64.203854
1696.412917	81.510898	64.208858
1695.700688	89.225834	64.213863
1695.067686	80.773798	64.218868
1695.011442	74.810088	64.223873
1693.847565	77.708161	64.228878
1693.502962	83.226360	64.233882
1692.588179	85.015701	64.238887
1692.291480	82.018589	64.243892
1691.308902	75.829812	64.248897
1690.575015	77.836433	64.253902
1690.264480	82.749978	64.258906
1689.364996	80.047282	64.263911
1688.128071	79.877153	64.268916
1687.444572	78.330767	64.273921
1687.228528	85.618403	64.278926
1686.895093	72.996628	64.283930
1686.434612	88.677817	64.288935
1685.442948	80.768441	64.293940
1684.471525	79.516937	64.298945
1683.706219	81.914905	64.303950
1683.783780	74.106982	64.308954
1682.852653	82.094798	64.313959
1681.841139	78.801189	64.318964
1681.083911	89.503729	64.323969
1680.593395	82.932463	64.328974
1680.378138	71.630764	64.333978
1679.081113	83.656932	64.338983
1678.517788	78.579574	64.343988
1677.685232	84.038064	64.348993
1677.558443	84.845988	64.353998
1677.015278	80.326826	64.359002
1676.276588	84.124064	64.364007
1675.150334	89.327997	64.369012
1674.580327	77.607964	64.374017
1674.081830	81.918996	64.379022
1674.110434	75.517612	64.384026
1672.787516	88.306416	64.389031
1672.439081	82.294488	64.394036
1671.614215	82.372747	64.399041
1670.714327	86.679713	64.404046
1669.621673	77.729820	64.409050
1668.802885	86.658594	64.414055
1668.655306	73.583107	64.419060
1668.003182	79.363030	64.424065
1667.303506	78.842666	64.429070
1667.065256	75.669119	64.434074
1666.531730	83.346217	64.439079
1665.344671	74.458629	64.444084
1664.983611	72.056796	64.449089
1664.537315	80.652024	64.454094
1663.893518	77.574418	64.459098
1662.506421	75.816497	64.464103
1662.051816	81.467284	64.469108
1661.748241	76.548955	64.474113
1661.015073	82.048437	64.479118
1660.509970	79.029232	64.484122
1659.289322	86.910069	64.489127
1658.746283	77.953325	64.494132
1658.510290	86.928322	64.499137
1657.489325	85.157990	64.504142
1656.784798	76.520208	64.509146
1655.888909	89.832564	64.514151
1655.766666	76.319388	64.519156
1655.077291	84.532173	64.524161
1654.517753	86.917973	64.529166
1654.080887	78.166720	64.534170
1652.979357	80.993408	64.539175
1652.439299	84.345944	64.544180
1651.274583	83.443695	64.549185
1650.257805	76.651660	64.554190
1649.846275	78.029932	64.559194
1649.458825	93.287941	64.564199
1649.157073	84.404841	64.569204
1648.883765	88.385225	64.574209
1647.944825	94.253285	64.579214
1647.183164	90.180414	64.584218
1646.337947	99.554947	64.589223
1645.588187	83.058463	64.594228
1645.393568	86.578493	64.599233
1644.252126	85.319311	64.604238
1643.838035	82.520623	64.609242
1643.168841	88.842586	64.614247
1642.433056	79.176861	64.619252
1641.491537	81.557094	64.624257
1640.825413	83.866782	64.629262
1640.555286	79.941359	64.634266
1639.997725	81.905798	64.639271
1638.985180	82.499577	64.644276
1638.278236	91.341212	64.649281
1637.478376	85.539754	64.654286
1637.431639	75.775643	64.659290
1636.999309	81.369278	64.664295
1636.192420	78.767015	64.669300
1635.417427	75.718139	64.674305
1634.393704	82.107444	64.679310
1633.465394	75.123172	64.684314
1632.521169	81.692241	64.689319
1632.169394	80.269806	64.694324
1631.820856	85.134197	64.699329
1631.504403	81.794876	64.704334
1631.172715	71.079385	64.709338
1630.239199	93.772748	64.714343
1629.594695	76.460043	64.719348
1628.498216	80.003455	64.724353
1627.345749	78.867457	64.729358
1626.960986	75.846495	64.734362
1625.992762	76.568858	64.739367
1625.998863	77.518105	64.744372
1625.604333	81.218118	64.749377
1624.772481	82.346179	64.754382
1624.037496	79.073331	64.759386
1623.040637	93.373140	64.764391
1622.825897	81.421655	64.769396
1622.168219	79.768684	64.774401
1620.739521	86.955600	64.779406
1620.688914	76.225427	64.784410
1619.737256	83.617277	64.789415
1619.409141	76.853079	64.794420
1619.212918	79.747310	64.799425
1617.733652	86.513325	64.804430
1617.532970	85.599908	64.809434
1616.663321	83.146391	64.814439
1615.966597	78.534938	64.819444
1615.080382	75.710315	64.824449
1614.387976	81.972889	64.829454
1614.260739	74.839319	64.834458
1613.607950	83.866319	64.839463
1612.764613	76.392317	64.844468
1611.954047	77.084914	64.849473
1611.029164	86.265518	64.854478
1611.059653	75.746396	64.859482
1610.223360	83.108886	64.864487
1609.029784	72.380477	64.869492
1608.452551	75.742077	64.874497
1607.867579	87.104824	64.879502
1607.947578	74.917300	64.884506
1606.836115	85.876386	64.889511
1605.936987	82.812540	64.894516
1605.360940	81.288534	64.899521
1604.985030	77.375187	64.904526
1604.380081	72.408541	64.909530
1602.786926	82.900080	64.914535
1602.626498	84.427712	64.919540
1602.342952	76.081056	64.924545
1601.574683	81.769052	64.929550
1600.890450	70.153925	64.934554
1599.762651	83.570929	64.939559
1599.377433	70.785515	64.944564
1599.074089	80.636956	64.949569
1598.399947	84.827663	64.954574
1597.691126	76.927024	64.959578
1596.687192	78.604398	64.964583
1596.510651	78.450397	64.969588
1595.807479	78.785318	64.974593
1594.679973	80.632132	64.979598
1594.336356	78.798398	64.984602
1593.891055	79.379369	64.989607
1593.024455	79.361778	64.994612
1591.870994	80.790090	64.999617
1591.233272	78.329708	65.004622
1590.901415	71.741154	65.009626
1590.308545	76.532389	65.014631
1589.595283	77.908131	65.019636
1588.765930	76.189395	65.024641
1587.966798	80.273799	65.029646
1587.988201	72.326568	65.034650
1587.187349	85.860383	65.039655
1586.201413	83.997783	65.044660
1585.271601	78.524495	65.049665
1584.880224	79.481681	65.054670
1584.782825	76.277887	65.059674
1583.708196	83.905323	65.064679
1583.103946	80.502912	65.069684
1582.635503	82.639288	65.074689
1581.476307	83.562312	65.079694
1580.842760	82.925811	65.084698
1579.731193	83.797115	65.089703
1579.677350	78.615205	65.094708
1579.260181	81.385259	65.099713
1578.697106	75.907341	65.104718
1577.687751	76.059088	65.109722
1576.541861	85.470346	65.114727
1576.137795	82.073987	65.119732
1575.702039	79.464835	65.124737
1575.453207	80.126566	65.129742
1574.313512	74.585697	65.134746
1573.499637	90.565871	65.139751
1573.158979	81.219035	65.144756
1572.860361	82.748117	65.149761
1571.943846	82.118718	65.154766
1571.136566	73.211860	65.159770
1570.336975	83.112163	65.164775
1569.781716	75.789541	65.169780
1569.057087	75.899219	65.174785
1567.972787	72.259251	65.179790
1567.655116	76.574690	65.184794
1567.196116	85.608763	65.189799
1566.938042	72.333228	65.194804
1566.027578	84.963512	65.199809
1565.018806	77.533154	65.204814
1564.932070	79.941639	65.209818
1563.431097	78.818451	65.214823
1562.793463	74.552446	65.219828
1562.439074	75.486412	65.224833
1561.587535	76.552964	65.229838
1561.171387	70.400431	65.234842
1560.936637	81.455233	65.239847
1560.198967	83.372603	65.244852
1559.292283	76.670356	65.249857
1558.589016	77.429505	65.254862
1557.713892	77.605669	65.259866
1556.638093	81.100090	65.264871
1556.169398	80.022669	65.269876
1555.540255	70.398393	65.274881
1555.202217	72.681215	65.279886
1555.232297	80.784464	65.284890
1553.863522	80.214294	65.289895
1553.274742	82.768760	65.294900
1552.555643	82.084354	65.299905
1552.283734	87.947410	65.304910
1551.423822	78.804488	65.309914
1550.494694	82.581544	65.314919
1550.052579	78.543105	65.319924
1549.682368	74.914294	65.324929
1548.769375	77.873499	65.329934
1547.973304	77.038895	65.334938
1547.158198	80.197018	65.339943
1546.946934	77.446555	65.344948
1546.464380	71.941664	65.349953
1545.015810	82.427610	65.354958
1544.918586	80.863828	65.359962
1543.942125	83.107716	65.364967
1542.988462	78.158632	65.369972
1542.626552	75.649720	65.374977
1541.944195	80.264367	65.379982
1541.596052	69.948905	65.384986
1540.610181	75.923793	65.389991
1539.788667	76.428916	65.394996
1539.441427	79.664108	65.400001
1538.833205	76.973549	65.405006
1538.546747	68.264673	65.410010
1537.452516	72.571006	65.415015
1536.578394	76.396098	65.420020
1536.145706	72.428706	65.425025
1535.482927	80.974753	65.430030
1534.801347	73.904022	65.435034
1533.713504	82.862947	65.440039
1533.175946	81.244534	65.445044
1533.118546	68.432297	65.450049
1532.176876	77.725968	65.455054
1531.332347	72.795824	65.460058
1530.675469	78.027746	65.465063
1530.464092	73.000177	65.470068
1529.900598	71.557774	65.475073
1528.613472	78.730124	65.480078
1528.284284	62.110139	65.485082
1527.525861	77.712489	65.490087
1526.573613	73.892289	65.495092
1525.613484	73.946349	65.500097
1524.995715	72.145139	65.505102
1524.939570	61.163557	65.510106
1524.268568	78.521366	65.515111
1524.074361	77.312037	65.520116
1523.099929	71.730748	65.525121
1521.782284	81.751204	65.530126
1521.699009	72.741968	65.535130
1521.085529	73.165164	65.540135
1520.337687	75.897868	65.545140
1519.322203	74.162993	65.550145
1518.701744	77.720712	65.555150
1518.362387	75.299684	65.560154
1518.012564	75.693611	65.565159
1517.449395	71.970880	65.570164
1516.367987	81.941194	65.575169
1515.800197	87.092738	65.580174
1514.875777	77.878078	65.585178
1514.064779	85.660776	65.590183
1513.644436	81.727695	65.595188
1513.498945	76.300152	65.600193
1511.897791	76.225815	65.605198
1511.333397	69.426637	65.610202
1511.019739	75.304206	65.615207
1510.590396	75.702882	65.620212
1510.022539	78.506346	65.625217
1508.388876	83.026122	65.630222
1508.358785	82.271695	65.635226
1507.456939	83.650609	65.640231
1507.291757	74.526652	65.645236
1506.705009	82.368342	65.650241
1505.606713	77.675639	65.655246
1505.076713	77.189865	65.660250
1504.715173	81.720437	65.665255
1503.818485	76.562045	65.670260
1502.928733	78.916752	65.675265
1502.135596	82.099783	65.680270
1502.191149	72.704217	65.685274
1501.071120	83.603192	65.690279
1500.210377	83.023305	65.695284
1499.618100	75.063186	65.700289
1499.250425	72.761779	65.705294
1498.684024	77.774329	65.710298
1497.617174	82.052676	65.715303
1497.015161	72.712691	65.720308
1496.519572	74.793467	65.725313
1496.104629	74.559075	65.730318
1495.014636	71.695908	65.735322
1494.185782	68.196742	65.740327
1493.649704	80.089468	65.745332
1493.712635	68.204296	65.750337
1492.796802	76.011533	65.755342
1491.886856	73.665389	65.760346
1490.999969	78.624777	65.765351
1490.813147	76.852882	65.770356
1489.790863	75.803498	65.775361
1488.657160	82.725987	65.780366
1488.449346	71.153486	65.785370
1487.695952	85.665373	65.790375
1487.565138	74.809191	65.795380
1486.650752	73.651203	65.800385
1485.617854	76.930676	65.805390
1485.074792	77.714854	65.810394
1484.830066	75.499572	65.815399
1484.230490	67.516967	65.820404
1483.028705	73.325901	65.825409
1482.150664	77.386597	65.830414
1482.299560	67.526774	65.835418
1481.693997	71.115248	65.840423
1480.512790	74.345745	65.845428
1480.328565	64.313344	65.850433
1479.408394	68.886935	65.855438
1478.506840	70.724705	65.860442
1477.381144	73.102712	65.865447
1477.112422	70.624738	65.870452
1476.711495	69.112365	65.875457
1476.128959	70.140936	65.880462
1475.723145	61.132494	65.885466
1474.483516	72.225513	65.890471
1473.861916	76.565591	65.895476
1473.599355	67.867124	65.900481
1472.885152	72.176182	65.905486
1471.802414	71.013408	65.910490
1470.963221	81.522419	65.915495
1470.742672	70.655268	65.920500
1470.477230	70.677826	65.925505
1469.289833	80.324370	65.930510
1469.013132	66.980860	65.935514
1468.079566	72.712492	65.940519
1467.309632	74.567202	65.945524
1466.268177	71.773606	65.950529
1465.546366	74.625191	65.955534
1465.517126	66.383244	65.960538
1465.089211	70.416583	65.965543
1464.653623	66.826561	65.970548
1463.716710	65.874011	65.975553
1462.757310	74.162841	65.980558
1462.327447	69.982127	65.985562
1461.021976	74.831409	65.990567
1460.381163	78.565838	65.995572
1460.226523	72.802287	66.000577
1459.814302	76.054118	66.005582
1459.534838	70.652599	66.010586
1458.492107	76.089343	66.015591
1457.840546	71.289417	66.020596
1456.962457	73.173928	66.025601
1455.561233	75.398602	66.030606
1455.333557	74.746532	66.035610
1454.859352	70.725829	66.040615
1454.443891	77.669830	66.045620
1453.626360	78.485007	66.050625
1452.278718	76.567967	66.055630
1452.178042	73.497168	66.060634
1451.647941	72.844264	66.065639
1451.392661	63.733061	66.070644
1450.435723	72.142927	66.075649
1449.609849	77.564142	66.080654
1448.863947	76.065584	66.085658
1447.597369	73.086991	66.090663
1447.242888	63.415963	66.095668
1447.019792	67.640687	66.100673
1446.514847	74.226743	66.105678
1445.944368	68.972391	66.110682
1444.814939	73.675437	66.115687
1444.187896	74.040880	66.120692
1443.818970	66.401688	66.125697
1442.962658	65.225027	66.130702
1442.161140	64.851793	66.135706
1441.260689	69.723461	66.140711
1440.998792	66.941633	66.145716
1440.599138	71.725846	66.150721
1439.741151	70.633031	66.155726
1439.258034	65.293838	66.160730
1438.350706	70.679110	66.165735
1437.819139	63.013723	66.170740
1437.299519	72.637749	66.175745
1436.014981	71.574863	66.180750
1435.733420	67.559827	66.185754
1435.104829	74.678041	66.190759
1434.588411	72.015501	66.195764
1433.469010	68.489982	66.200769
1432.613805	71.939936	66.205774
1432.200454	69.574835	66.210778
1431.884371	75.041208	66.215783
1431.266665	73.142240	66.220788
1430.475948	63.953692	66.225793
1429.465964	77.832990	66.230798
1429.514438	72.292636	66.235802
1428.749284	75.912786	66.240807
1427.730915	80.787429	66.245812
1427.072451	74.865815	66.250817
1426.323203	82.963572	66.255822
1426.070505	74.976327	66.260826
1424.665194	77.651098	66.265831
1424.081923	75.771891	66.270836
1423.954308	74.438450	66.275841
1423.252942	75.813920	66.280846
1422.995059	73.829395	66.285850
1421.614163	76.803063	66.290855
1421.008736	68.163817	66.295860
1420.786257	69.031109	66.300865
1420.067848	75.149616	66.305870
1419.328807	68.458640	66.310874
1418.522637	69.749840	66.315879
1417.805766	75.415516	66.320884
1416.907202	70.834624	66.325889
1415.991519	79.163831	66.330894
1415.672381	68.206703	66.335898
1415.262867	65.069865	66.340903
1414.973919	66.723581	66.345908
1414.672754	65.781994	66.350913
1413.238234	78.743158	66.355918
1412.726985	69.612709	66.360922
1411.978420	74.927031	66.365927
1411.030990	73.679704	66.370932
1410.339820	75.222292	66.375937
1409.613676	67.069011	66.380942
1409.841923	69.698681	66.385946
1408.691188	67.393985	66.390951
1408.073405	72.594486	66.395956
1407.637349	67.496981	66.400961
1406.750869	78.844572	66.405966
1406.064186	66.793096	66.410970
1405.022555	73.021313	66.415975
1404.523948	67.746090	66.420980
1404.289931	74.342716	66.425985
1403.117634	78.085917	66.430990
1402.442992	70.783894	66.435994
1401.626933	76.652994	66.440999
1401.534935	75.383279	66.446004
1401.241946	78.236126	66.451009
1400.086327	84.678004	66.456014
1399.462208	79.673459	66.461018
1398.736019	83.467201	66.466023
1397.949007	78.873318	66.471028
1396.959238	76.748052	66.476033
1396.251024	80.013810	66.481038
1396.080886	73.632986	66.486042
1395.630684	80.714977	66.491047
1395.062615	72.121840	66.496052
1394.338840	74.773482	66.501057
1393.374015	84.545536	66.506062
1393.500212	72.319157	66.511066
1392.128764	78.793756	66.516071
1391.274507	78.081987	66.521076
1390.930050	74.540575	66.526081
1389.798094	78.772535	66.531086
1388.791766	72.034157	66.536090
1388.501181	77.490174	66.541095
1388.331135	74.086628	66.546100
1387.765009	73.144570	66.551105
1386.924786	80.998170	66.556110
1386.333128	77.168034	66.561114
1385.185598	84.572153	66.566119
1384.474675	74.035255	66.571124
1384.190913	83.440463	66.576129
1383.987597	82.666256	66.581134
1383.147616	76.535380	66.586138
1382.164947	84.290193	66.591143
1381.667672	77.740581	66.596148
1380.948532	78.437643	66.601153
1379.880426	79.136543	66.606158
1379.513256	76.540184	66.611162
1378.980550	83.971181	66.616167
1378.461007	78.287702	66.621172
1377.402614	78.570321	66.626177
1376.404639	85.994832	66.631182
1376.328690	79.050259	66.636186
1375.911554	79.568442	66.641191
1375.177584	77.957623	66.646196
1374.058369	76.728147	66.651201
1373.313436	83.675629	66.656206
1373.526675	77.304845	66.661210
1372.226947	76.556641	66.666215
1371.375396	76.271805	66.671220
1370.910636	70.158579	66.676225
1370.210492	83.113447	66.681230
1370.091476	73.788211	66.686234
1368.713397	75.760092	66.691239
1368.147978	80.692084	66.696244
1368.117735	72.141219	66.701249
1367.362203	78.440679	66.706254
1366.466995	77.330150	66.711258
1365.542244	75.692882	66.716263
1365.038936	70.306451	66.721268
1364.781920	73.372779	66.726273
1363.634097	75.901006	66.731278
1363.007016	74.388322	66.736282
1361.998317	80.841558	66.741287
1361.627493	68.339356	66.746292
1361.468703	77.713660	66.751297
1360.675189	78.944519	66.756302
1360.170048	73.880078	66.761306
1358.564774	75.241519	66.766311
1357.800793	70.841112	66.771316
1357.369433	62.587389	66.776321
1356.815459	77.548564	66.781326
1356.615242	72.139199	66.786330
1356.233829	76.322857	66.791335
1355.591675	77.222157	66.796340
1354.737621	78.399560	66.801345
1353.996900	77.877919	66.806350
1353.038022	74.711702	66.811354
1351.970174	73.478804	66.816359
1351.211486	67.317678	66.821364
1351.138306	75.432583	66.826369
1350.566464	77.793584	66.831374
1350.471956	74.791199	66.836378
1349.454170	85.221387	66.841383
1348.501571	83.755707	66.846388
1348.221769	77.960019	66.851393
1346.945994	74.777936	66.856398
1346.650207	75.213760	66.861402
1346.050540	78.812363	66.866407
1345.514032	75.440252	66.871412
1343.866605	68.333851	66.876417
1343.279521	75.839722	66.881422
1343.073852	64.449842	66.886426
1342.372623	78.636483	66.891431
1342.399880	74.174987	66.896436
1341.761327	69.092332	66.901441
1340.627193	76.601566	66.906446
1340.113953	75.231645	66.911450
1339.280568	79.357826	66.916455
1338.188981	78.888798	66.921460
1337.679114	72.421625	66.926465
1337.260043	79.765179	66.931470
1336.910253	84.505212	66.936474
1336.012956	83.131673	66.941479
1335.416465	75.161236	66.946484
1334.703820	83.746781	66.951489
1334.101691	86.188295	66.956494
1333.926642	78.056260	66.961498
1332.537759	77.084126	66.966503
1332.209146	77.671826	66.971508
1331.853102	85.081060	66.976513
1330.165455	82.082714	66.981518
1329.970181	76.065438	66.986522
1329.478246	72.872328	66.991527
1329.103744	79.723098	66.996532
1327.900609	76.546825	67.001537
1326.736081	70.101702	67.006542
1326.375132	73.797985	67.011546
1325.972582	82.834141	67.016551
1325.869810	68.805432	67.021556
1325.326289	71.213976	67.026561
1324.351091	85.007352	67.031566
1323.540008	72.852673	67.036570
1322.388583	72.664398	67.041575
1321.452299	75.912805	67.046580
1321.223640	72.731470	67.051585
1320.980472	72.304225	67.056590
1320.330527	72.223905	67.061594
1319.376933	75.047710	67.066599
1318.779748	70.718578	67.071604
1318.467597	75.566167	67.076609
1317.586937	80.179263	67.081614
1316.859755	73.707211	67.086618
1315.961429	77.807449	67.091623
1315.403516	72.926450	67.096628
1315.336773	76.274777	67.101633
1314.239231	81.389122	67.106638
1313.388655	68.371826	67.111642
1312.764110	72.660363	67.116647
1312.252739	77.916509	67.121652
1311.884542	75.902221	67.126657
1310.461588	80.363390	67.131662
1310.082365	74.592973	67.136666
1309.806314	78.736237	67.141671
1308.982528	76.652434	67.146676
1308.331992	81.894431	67.151681
1307.468491	76.730842	67.156686
1307.355218	71.810713	67.161690
1306.071393	78.288771	67.166695
1305.130633	81.039578	67.171700
1304.768845	78.027637	67.176705
1303.923615	83.669588	67.181710
1303.836966	79.350775	67.186714
1303.511646	73.188593	67.191719
1302.509773	84.209199	67.196724
1301.868693	76.408286	67.201729
1300.793658	76.731427	67.206734
1299.784698	73.708810	67.211738
1299.185633	77.936531	67.216743
1298.741419	70.206833	67.221748
1298.547954	71.438530	67.226753
1298.203877	77.589028	67.231758
1297.403802	70.694908	67.236762
1296.479839	77.234043	67.241767
1295.789558	72.077620	67.246772
1294.956773	73.210661	67.251777
1293.899161	74.504016	67.256782
1293.746144	72.140138	67.261786
1293.292929	78.074595	67.266791
1292.599921	78.313364	67.271796
1291.599390	75.633187	67.276801
1290.786008	77.174729	67.281806
1290.570867	75.293812	67.286810
1290.089525	80.447419	67.291815
1288.679661	82.153157	67.296820
1288.432512	77.918204	67.301825
1287.685917	79.384478	67.306830
1287.501789	62.769894	67.311834
1286.305872	76.486389	67.316839
1285.647202	81.806954	67.321844
1285.568313	74.430775	67.326849
1284.837983	77.941349	67.331854
1283.506211	75.515675	67.336858
1283.140058	71.138792	67.341863
1282.452456	67.604634	67.346868
1282.321542	69.599095	67.351873
1281.106365	75.974788	67.356878
1280.796551	70.586008	67.361882
1280.124284	76.701940	67.366887
1279.174205	72.750610	67.371892
1278.663040	73.537643	67.376897
1277.808758	77.009573	67.381902
1276.894064	66.598153	67.386906
1276.077949	70.549716	67.391911
1275.484332	74.115831	67.396916
1275.306866	69.138101	67.401921
1274.658191	81.096049	67.406926
1274.651996	62.185528	67.411930
1272.925541	71.903627	67.416935
1272.183474	67.253762	67.421940
1272.174964	65.492968	67.426945
1271.380998	73.132658	67.431950
1270.610211	71.702764	67.436954
1270.053336	74.203328	67.441959
1269.506002	77.132883	67.446964
1268.761268	71.590887	67.451969
1267.452114	77.913715	67.456974
1267.354841	69.882873	67.461978
1266.816672	77.544984	67.466983
1266.146916	76.855969	67.471988
1265.233891	73.335570	67.476993
1264.432884	78.059021	67.481998
1264.248358	69.537424	67.487002
1263.086046	72.320307	67.492007
1262.222077	73.869899	67.497012
1261.892820	63.900015	67.502017
1261.176271	72.139257	67.507022
1260.696067	58.358224	67.512026
1260.387155	64.690787	67.517031
1259.221353	62.890027	67.522036
1259.165083	65.908681	67.527041
1258.353773	72.655421	67.532046
1257.512171	64.541051	67.537050
1256.238261	74.045299	67.542055
1255.696744	72.583696	67.547060
1255.458084	69.836045	67.552065
1254.960339	82.662560	67.557070
1254.006821	78.601398	67.562074
1253.223379	71.690458	67.567079
1252.825337	69.867004	67.572084
1252.434533	68.860839	67.577089
1251.211526	74.471388	67.582094
1250.558603	62.031412	67.587098
1250.333041	72.933350	67.592103
1249.750925	66.677961	67.597108
1248.786120	67.992851	67.602113
1248.062807	74.801300	67.607118
1247.412145	69.498248	67.612122
1247.096506	73.666730	67.617127
1246.474984	67.619456	67.622132
1245.614866	74.648348	67.627137
1244.673410	76.588732	67.632142
1244.043980	63.318700	67.637146
1243.014046	70.995905	67.642151
1242.426852	62.561980	67.647156
1242.237628	66.782905	67.652161
1241.740339	70.308481	67.657166
1241.415430	71.182607	67.662170
1240.318144	74.921835	67.667175
1239.542579	76.031604	67.672180
1239.249838	67.230747	67.677185
1238.354533	71.844614	67.682190
1237.385338	66.291004	67.687194
1236.759795	62.680764	67.692199
1236.279551	69.546768	67.697204
1235.791711	71.186386	67.702209
1234.568734	75.730919	67.707214
1234.063105	78.915625	67.712218
1233.565981	74.174794	67.717223
1233.215033	67.414307	67.722228
1232.203252	68.785555	67.727233
1231.181543	74.670041	67.732238
1231.298608	69.246526	67.737242
1230.612071	68.823540	67.742247
1229.719745	68.387537	67.747252
1229.215008	65.906115	67.752257
1228.229250	65.705738	67.757262
1227.799192	66.626543	67.762266
1226.766065	73.742868	67.767271
1226.024935	62.464944	67.772276
1225.791828	61.298097	67.777281
1225.021978	66.888655	67.782286
1224.666832	68.381024	67.787290
1223.677962	71.085888	67.792295
1222.863787	65.126019	67.797300
1222.874625	63.808427	67.802305
1221.270397	67.825369	67.807310
1220.974828	63.369470	67.812314
1220.395211	69.010212	67.817319
1219.980036	66.632825	67.822324
1219.186098	59.177947	67.827329
1218.085535	74.965609	67.832334
1217.649895	70.133007	67.837338
1217.309297	65.728421	67.842343
1216.475402	69.868907	67.847348
1215.877340	61.953958	67.852353
1214.852098	68.414596	67.857358
1214.862395	64.195501	67.862362
1213.805182	63.320516	67.867367
1212.851971	66.038638	67.872372
1212.274399	58.095204	67.877377
1212.063457	69.248703	67.882382
1211.594927	62.831767	67.887386
1210.463574	69.574203	67.892391
1209.829629	57.183270	67.897396
1209.678496	66.357647	67.902401
1208.263148	63.964226	67.907406
1207.351617	63.711057	67.912410
1206.890783	66.730948	67.917415
1206.405050	68.430160	67.922420
1206.313116	61.672658	67.927425
1205.081413	67.432840	67.932430
1204.230270	63.727588	67.937434
1203.993642	69.808967	67.942439
1203.280376	68.560762	67.947444
1202.707745	65.587092	67.952449
1201.614068	62.459716	67.957454
1201.270773	65.300073	67.962458
1200.523349	71.822205	67.967463
1200.199156	60.597856	67.972468
1199.223318	63.032575	67.977473
1198.505365	62.105237	67.982478
1198.243771	57.066779	67.987482
1197.080733	67.356086	67.992487
1196.031736	64.153800	67.997492
1195.927486	56.234470	68.002497
1195.318832	60.783850	68.007502
1195.094599	61.742900	68.012506
1194.331159	69.030822	68.017511
1193.493787	66.250631	68.022516
1193.260736	59.502951	68.027521
1191.587525	68.774236	68.032526
1190.973471	59.223388	68.037530
1190.658608	60.546930	68.042535
1190.148396	69.053000	68.047540
1189.678087	60.485393	68.052545
1188.472647	64.478375	68.057550
1187.733437	66.096464	68.062554
1187.315511	61.836642	68.067559
1186.678638	62.098053	68.072564
1186.273138	56.989436	68.077569
1185.216045	64.316160	68.082574
1184.492100	62.661228	68.087578
1184.347298	62.901177	68.092583
1183.328725	65.183423	68.097588
1182.818774	62.179293	68.102593
1181.708930	72.628886	68.107598
1181.742303	65.666959	68.112602
1180.941553	69.483641	68.117607
1180.140866	61.436916	68.122612
1179.708840	56.886027	68.127617
1178.591131	60.078166	68.132622
1178.364613	58.962315	68.137626
1177.570531	71.295045	68.142631
1176.789360	62.833634	68.147636
1176.585167	55.163586	68.152641
1175.130785	60.367825	68.157646
1174.438483	63.520716	68.162650
1174.054498	69.862068	68.167655
1173.581595	60.350284	68.172660
1173.191152	66.566505	68.177665
1172.142403	73.174398	68.182670
1171.732097	60.538185	68.187674
1171.005946	59.851855	68.192679
1170.078460	63.073679	68.197684
1169.547990	57.150727	68.202689
1168.483324	69.327783	68.207694
1168.322181	62.750022	68.212698
1167.897572	64.366981	68.217703
1166.814093	58.593456	68.222708
1166.724860	66.373429	68.227713
1165.625709	63.291094	68.232718
1164.453987	54.928058	68.237722
1163.882733	65.599523	68.242727
1163.002703	60.810785	68.247732
1163.143818	57.895531	68.252737
1162.615723	65.144463	68.257742
1162.027483	56.952006	68.262746
1161.132850	63.152197	68.267751
1160.537250	59.923571	68.272756
1159.794624	52.069478	68.277761
1158.473266	67.890675	68.282766
1158.027755	57.231254	68.287770
1157.471992	59.340576	68.292775
1157.148969	57.651869	68.297780
1156.265035	57.602487	68.302785
1155.561176	67.254252	68.307790
1155.108341	60.890029	68.312794
1154.538044	70.168900	68.317799
1153.628410	68.810005	68.322804
1153.144761	63.914090	68.327809
1152.292917	69.184967	68.332814
1151.972312	63.849967	68.337818
1151.172093	60.923536	68.342823
1150.115967	58.514034	68.347828
1150.022087	63.434158	68.352833
1149.247349	65.906305	68.357838
1148.218395	65.097817	68.362842
1147.523365	60.814255	68.367847
1147.043921	55.154433	68.372852
1147.211323	56.374490	68.377857
1145.372922	59.656002	68.382862
1144.832332	61.157366	68.387866
1144.221117	58.150423	68.392871
1143.502173	69.685890	68.397876
1143.492097	56.055651	68.402881
1142.371224	60.763756	68.407886
1141.614247	59.932526	68.412890
1141.329488	60.415503	68.417895
1140.687120	71.180283	68.422900
1139.667734	65.262537	68.427905
1138.766269	65.923999	68.432910
1138.745243	57.116236	68.437914
1138.367978	63.954834	68.442919
1137.320968	64.604746	68.447924
1136.831664	62.168199	68.452929
1135.870091	69.057131	68.457934
1134.809628	72.774774	68.462938
1134.204128	54.361708	68.467943
1133.468978	69.465233	68.472948
1133.138295	59.642266	68.477953
1132.910679	74.548401	68.482958
1132.424769	54.600870	68.487962
1131.456634	67.142629	68.492967
1130.744555	61.560800	68.497972
1129.821131	57.792953	68.502977
1128.683228	71.124954	68.507982
1128.402934	64.883110	68.512986
1128.139851	64.777595	68.517991
1127.615551	67.094809	68.522996
1126.809259	59.954167	68.528001
1125.859447	53.463975	68.533006
1125.566910	60.205522	68.538010
1124.472025	70.356285	68.543015
1123.474194	64.791510	68.548020
1123.063472	62.916480	68.553025
1122.428975	63.120759	68.558030
1122.357026	54.041976	68.563034
1121.845811	60.103938	68.568039
1120.451777	62.076904	68.573044
1120.406673	54.446223	68.578049
1119.452795	65.954393	68.583054
1118.441232	55.853348	68.588058
1117.955497	60.496737	68.593063
1117.454300	52.643692	68.598068
1117.001892	58.209026	68.603073
1115.579771	62.548730	68.608078
1115.217607	50.936211	68.613082
1114.735216	61.678702	68.618087
1114.268890	68.525159	68.623092
1113.233766	58.874137	68.628097
1112.220460	56.437343	68.633102
1112.001288	69.129670	68.638106
1111.653906	61.767826	68.643111
1110.977614	59.099245	68.648116
1109.961810	55.519562	68.653121
1109.277775	63.976007	68.658126
1108.781803	61.881147	68.663130
1108.494499	63.223970	68.668135
1107.742163	62.451936	68.673140
1107.199874	57.456550	68.678145
1106.218615	67.847869	68.683150
1105.398640	61.808544	68.688154
1104.550455	62.595585	68.693159
1103.805897	64.315471	68.698164
1103.716632	63.527884	68.703169
1102.866131	65.980552	68.708174
1101.808234	64.331441	68.713178
1101.211379	59.672738	68.718183
1100.730712	64.160783	68.723188
1100.708994	58.267335	68.728193
1099.630131	62.397921	68.733198
1098.766093	56.909654	68.738202
1098.313078	63.485913	68.743207
1097.833614	60.590494	68.748212
1096.995616	62.115507	68.753217
1096.025928	61.896856	68.758222
1095.541017	65.409447	68.763226
1095.138454	64.302675	68.768231
1094.188339	60.458662	68.773236
1093.687503	65.195920	68.778241
1093.340667	62.649994	68.783246
1092.401511	68.231238	68.788250
1091.183609	76.895592	68.793255
1090.477751	69.013592	68.798260
1090.293341	71.194761	68.803265
1089.645234	77.382582	68.808270
1089.081047	63.559764	68.813274
1088.198377	70.300545	68.818279
1087.826721	62.031090	68.823284
1087.247564	57.897855	68.828289
1086.372388	63.828468	68.833294
1085.439483	66.822524	68.838298
1085.073680	58.985801	68.843303
1084.599687	67.686393	68.848308
1083.871697	64.901462	68.853313
1082.779269	76.778611	68.858318
1082.673631	65.517955	68.863322
1081.817414	68.157619	68.868327
1080.592820	71.619109	68.873332
1080.177158	53.888659	68.878337
1079.585330	77.671004	68.883342
1079.449143	65.019607	68.888346
1078.360931	68.702258	68.893351
1077.284530	68.745012	68.898356
1076.957364	65.563604	68.903361
1076.123045	67.275696	68.908366
1076.063967	56.072299	68.913370
1074.995321	59.873263	68.918375
1074.152934	69.493456	68.923380
1073.819957	65.838312	68.928385
1073.428708	68.738348	68.933390
1072.582063	55.100811	68.938394
1071.853753	72.092442	68.943399
1071.076942	68.454264	68.948404
1070.949290	67.034119	68.953409
1069.624725	70.405856	68.958414
1069.038085	64.102355	68.963418
1068.313690	65.282882	68.968423
1067.970306	62.555063	68.973428
1067.402066	61.201833	68.978433
1066.370206	70.046340	68.983438
1066.140347	55.690977	68.988442
1065.428463	61.466316	68.993447
1064.341257	71.220064	68.998452
1064.025134	64.974468	69.003457
1063.196182	67.341720	69.008462
1062.754205	61.081448	69.013466
1061.712366	67.760817	69.018471
1060.889196	65.722734	69.023476
1060.653505	63.931842	69.028481
1060.058620	70.797174	69.033486
1059.174352	64.758628	69.038490
1058.201801	67.419954	69.043495
1057.669380	63.244600	69.048500
1057.776965	60.195905	69.053505
1056.623277	64.896646	69.058510
1055.805134	69.528257	69.063514
1055.648308	70.229017	69.068519
1054.592551	65.263263	69.073524
1053.938337	68.570974	69.078529
1052.769350	74.830602	69.083534
1052.667708	68.077811	69.088538
1052.128047	70.569369	69.093543
1051.576232	66.095902	69.098548
1051.001961	60.979460	69.103553
1049.707894	69.818366	69.108558
1049.073292	66.351543	69.113562
1048.938377	60.487140	69.118567
1047.736802	72.848431	69.123572
1047.427327	62.779259	69.128577
1046.629611	73.687030	69.133582
1046.579226	66.047729	69.138586
1045.485753	62.614464	69.143591
1044.434898	67.054430	69.148596
1043.946086	68.079225	69.153601
1043.298698	74.120283	69.158606
1042.798204	63.136899	69.163610
1042.004938	75.390678	69.168615
1041.830649	67.905123	69.173620
1040.834652	61.701430	69.178625
1039.556947	65.083075	69.183630
1039.010791	63.874571	69.188634
1038.721123	64.061874	69.193639
1038.345898	57.068751	69.198644
1038.165152	61.231561	69.203649
1036.838491	68.872444	69.208654
1036.163861	61.762936	69.213658
1035.393806	64.906148	69.218663
1034.289464	68.168760	69.223668
1034.159612	69.511780	69.228673
1033.545395	66.838079	69.233678
1033.185019	66.464196	69.238682
1031.909150	68.408954	69.243687
1030.934599	76.246153	69.248692
1030.768640	67.921915	69.253697
1030.221731	69.763350	69.258702
1029.851491	73.823838	69.263706
1028.629540	67.165655	69.268711
1027.975810	70.542681	69.273716
1027.643434	57.477804	69.278721
1026.959125	72.529104	69.283726
1026.025749	63.839649	69.288730
1025.614479	67.562887	69.293735
1024.846938	72.557041	69.298740
1024.919740	64.603260	69.303745
1023.578989	62.215428	69.308750
1022.945214	64.486994	69.313754
1022.411193	73.463646	69.318759
1021.605952	72.468241	69.323764
1020.853324	64.803440	69.328769
1020.334641	70.360407	69.333774
1019.919839	68.937051	69.338778
1018.987294	75.774096	69.343783
1018.207923	68.417899	69.348788
1017.609379	68.720563	69.353793
1017.166989	63.305611	69.358798
1016.295444	66.876554	69.363802
1015.970706	67.041053	69.368807
1014.907831	67.130567	69.373812
1014.281857	63.211376	69.378817
1012.975284	71.090348	69.383822
1012.487099	63.905461	69.388826
1012.083545	72.091812	69.393831
1011.737844	79.893653	69.398836
1011.391240	61.212373	69.403841
1010.478479	69.107555	69.408846
1009.794007	69.676200	69.413850
1009.308991	65.135350	69.418855
1008.235463	69.063274	69.423860
1007.626519	62.287102	69.428865
1006.570181	70.517358	69.433870
1006.439749	69.064543	69.438874
1006.275596	72.283279	69.443879
1004.821043	68.062220	69.448884
1004.505446	57.511489	69.453889
1003.683051	59.146012	69.458894
1003.406346	54.657188	69.463898
1002.654761	58.560712	69.468903
1001.616245	57.173489	69.473908
1001.050564	59.779580	69.478913
1000.554135	65.150082	69.483918
999.857755	64.031713	69.488922
999.115440	65.057415	69.493927
998.270590	66.105733	69.498932
998.145831	61.638471	69.503937
997.113898	67.037382	69.508942
996.147051	63.571383	69.513946
995.476232	60.271187	69.518951
994.795540	68.840663	69.523956
994.925725	65.512405	69.528961
993.877598	71.968872	69.533966
992.904388	61.467549	69.538970
992.908324	69.333619	69.543975
992.137476	69.091264	69.548980
991.166183	66.843377	69.553985
990.377375	72.167350	69.558990
989.891849	66.025984	69.563994
989.580777	70.950692	69.568999
988.634609	73.981584	69.574004
988.060205	65.749130	69.579009
987.253398	66.190584	69.584014
986.470373	68.355012	69.589018
985.380956	64.446469	69.594023
984.909507	70.418549	69.599028
984.411699	65.588005	69.604033
983.960700	74.617688	69.609038
984.075318	71.343944	69.614042
983.015774	67.375456	69.619047
982.083655	73.321467	69.624052
981.346621	60.920207	69.629057
980.233336	60.440592	69.634062
979.647214	66.921342	69.639066
979.386543	65.438784	69.644071
978.755757	75.861125	69.649076
978.459056	67.092493	69.654081
977.327777	71.015423	69.659086
977.034071	70.708213	69.664090
976.246246	64.763170	69.669095
974.994664	62.879996	69.674100
974.945196	62.554437	69.679105
973.942468	69.754314	69.684110
973.565724	56.668125	69.689114
972.225451	56.786013	69.694119
971.558992	60.668119	69.699124
971.159331	62.512950	69.704129
970.973745	66.093063	69.709134
970.403036	58.560195	69.714138
969.746054	60.472766	69.719143
969.032145	60.159861	69.724148
968.087989	64.067219	69.729153
966.567800	62.143198	69.734158
966.580612	61.506536	69.739162
966.298998	58.999142	69.744167
965.720975	56.392243	69.749172
965.225364	50.812310	69.754177
964.090466	70.901091	69.759182
963.387936	71.335426	69.764186
962.930647	65.246346	69.769191
961.843736	65.246665	69.774196
961.339170	62.738467	69.779201
960.571632	73.832265	69.784206
960.444629	71.577818	69.789210
959.877839	68.693166	69.794215
958.687927	68.877028	69.799220
958.343929	65.015499	69.804225
957.579437	70.900158	69.809230
957.065176	60.832045	69.814234
956.214667	65.273288	69.819239
955.241515	66.845076	69.824244
955.451821	67.039586	69.829249
954.192872	71.036450	69.834254
953.238376	57.972788	69.839258
952.710193	60.361612	69.844263
952.417665	65.152484	69.849268
951.860258	59.237030	69.854273
950.808887	63.057371	69.859278
950.191456	60.865173	69.864282
950.134834	62.729553	69.869287
948.524445	67.231755	69.874292
948.412337	67.791366	69.879297
947.559309	70.563028	69.884302
947.193244	61.821209	69.889306
946.094284	61.087018	69.894311
945.257298	62.463684	69.899316
944.869680	51.743080	69.904321
944.046451	70.643731	69.909326
944.191936	62.618470	69.914330
943.241687	66.115223	69.919335
942.107521	75.466476	69.924340
941.873742	64.276692	69.929345
940.980455	66.862372	69.934350
939.823275	67.807431	69.939354
939.414703	67.207841	69.944359
938.720803	64.034334	69.949364
938.459215	62.820007	69.954369
938.063275	73.398957	69.959374
937.455468	64.134203	69.964378
936.829752	65.305375	69.969383
935.796148	70.215720	69.974388
935.043859	63.984343	69.979393
934.433461	62.377654	69.984398
934.236385	61.786997	69.989402
933.045027	65.733693	69.994407
931.956546	70.942928	69.999412
931.887407	60.234734	70.004417
931.221642	67.070359	70.009422
930.505367	68.787370	70.014426
929.816604	64.084988	70.019431
928.946923	62.568434	70.024436
928.847135	58.712216	70.029441
927.678400	64.946617	70.034446
926.951597	75.839978	70.039450
926.505505	69.052112	70.044455
925.862572	75.352679	70.049460
925.578038	54.509031	70.054465
924.112242	66.756274	70.059470
923.556196	61.425658	70.064474
923.248620	60.037300	70.069479
922.581508	70.213113	70.074484
921.804393	55.935385	70.079489
920.808934	73.114611	70.084494
920.492755	66.214618	70.089498
920.319034	67.998280	70.094503
919.327005	65.771068	70.099508
918.518327	64.087118	70.104513
917.749390	61.575258	70.109518
917.661608	65.518279	70.114522
916.635388	65.643002	70.119527
915.723085	60.176678	70.124532
915.483678	61.912443	70.129537
914.626650	63.628196	70.134542
913.321774	56.131724	70.139546
912.942152	67.452392	70.144551
912.371800	70.877679	70.149556
912.282392	50.692122	70.154561
911.892258	61.244909	70.159566
910.820559	67.255723	70.164570
910.081099	57.874733	70.169575
909.451519	63.849900	70.174580
908.191851	59.675168	70.179585
907.749193	65.093898	70.184590
906.761316	58.567279	70.189594
906.827831	63.138606	70.194599
906.240116	74.974932	70.199604
905.582570	53.462087	70.204609
904.824481	63.691795	70.209614
904.313260	62.922462	70.214618
903.251550	63.164801	70.219623
901.886354	69.919322	70.224628
901.830219	63.651318	70.229633
901.263915	74.000332	70.234638
901.088068	65.434839	70.239642
900.719718	61.580349	70.244647
899.395929	65.005660	70.249652
899.239403	61.183701	70.254657
898.098675	68.653138	70.259662
896.542605	67.840307	70.264666
896.630022	71.036368	70.269671
895.787068	75.105846	70.274676
895.840787	68.754131	70.279681
895.109112	68.726345	70.284686
894.062865	61.724895	70.289690
893.754890	65.986799	70.294695
892.664702	61.264719	70.299700
892.192499	61.432194	70.304705
891.251055	67.587870	70.309710
890.949980	62.642471	70.314714
890.379746	62.314613	70.319719
889.263972	66.716078	70.324724
888.629117	61.038466	70.329729
887.803243	60.328661	70.334734
887.718014	57.955612	70.339738
887.299262	60.644002	70.344743
886.303592	69.859696	70.349748
885.941425	61.025810	70.354753
885.039145	66.035125	70.359758
883.906466	57.158253	70.364762
883.477209	56.610849	70.369767
882.812619	62.017583	70.374772
882.547439	60.838527	70.379777
881.284762	67.160432	70.384782
880.672101	55.119476	70.389786
880.391544	61.168425	70.394791
880.126815	62.406753	70.399796
879.046865	61.503988	70.404801
877.914564	66.969370	70.409806
877.789769	71.375596	70.414810
877.067564	67.038094	70.419815
875.724843	63.628796	70.424820
875.665680	61.964378	70.429825
874.919763	68.219836	70.434830
874.293404	66.464315	70.439834
874.054078	55.817903	70.444839
872.871397	61.625614	70.449844
872.218851	61.225702	70.454849
872.007738	63.486822	70.459854
871.158278	54.762014	70.464858
870.351288	58.370036	70.469863
869.528465	66.804452	70.474868
869.259672	60.010473	70.479873
867.814164	59.113837	70.484878
867.535809	61.248462	70.489882
867.170556	58.401154	70.494887
866.526978	69.804824	70.499892
865.426782	57.696364	70.504897
864.477182	67.830398	70.509902
863.993462	69.518309	70.514906
863.852912	60.098813	70.519911
863.167547	69.301410	70.524916
863.351949	62.774365	70.529921
861.834376	71.002362	70.534926
861.347349	64.730382	70.539930
860.543523	61.156500	70.544935
859.413912	72.050884	70.549940
859.398861	59.821803	70.554945
858.578359	66.694678	70.559950
857.423714	59.899728	70.564954
856.904898	59.775007	70.569959
856.343987	67.792440	70.574964
856.222879	56.748754	70.579969
855.321431	65.119989	70.584974
854.397602	63.514307	70.589978
853.894181	58.009758	70.594983
853.382258	67.246259	70.599988
852.326372	59.257619	70.604993
851.425048	55.732372	70.609998
850.988953	52.098407	70.615002
850.357351	55.359984	70.620007
850.177488	64.106833	70.625012
849.462153	62.562595	70.630017
848.758620	66.016969	70.635022
848.138290	69.525913	70.640026
847.221198	59.022042	70.645031
846.210405	65.004263	70.650036
845.763962	59.763461	70.655041
845.085388	63.757909	70.660046
844.741739	61.033323	70.665050
844.140433	57.381492	70.670055
843.168619	63.683938	70.675060
842.936643	56.202867	70.680065
842.016637	59.440952	70.685070
840.593658	65.025140	70.690074
840.160874	71.262320	70.695079
839.656012	67.404331	70.700084
839.626269	60.748936	70.705089
839.194615	64.043357	70.710094
838.202446	64.150078	70.715098
837.591319	60.586542	70.720103
836.663153	67.586941	70.725108
835.804710	61.678419	70.730113
834.949865	61.455786	70.735118
834.443875	69.224788	70.740122
834.313299	63.284024	70.745127
833.492709	69.278562	70.750132
832.905276	61.371507	70.755137
832.076809	63.242013	70.760142
831.427534	58.796731	70.765146
830.873555	53.994089	70.770151
829.382748	63.622896	70.775156
829.521219	58.624912	70.780161
828.756520	63.426272	70.785166
828.028229	58.192477	70.790170
827.329021	52.785323	70.795175
826.568740	55.237910	70.800180
826.315093	54.672033	70.805185
825.630745	57.051036	70.810190
824.800591	67.724312	70.815194
824.259008	57.778862	70.820199
823.337426	70.392136	70.825204
822.669849	58.508170	70.830209
821.475151	59.083938	70.835214
821.112291	60.213309	70.840218
820.688863	60.401421	70.845223
820.338024	68.662972	70.850228
819.963247	50.768419	70.855233
818.886923	66.101309	70.860238
818.407207	62.581522	70.865242
817.871770	60.668046	70.870247
816.528687	66.100762	70.875252
816.068733	67.879515	70.880257
815.918057	64.608564	70.885262
814.947175	64.237247	70.890266
814.089290	60.162632	70.895271
813.372029	69.856011	70.900276
813.189244	52.813994	70.905281
812.013351	67.050987	70.910286
811.162961	66.480725	70.915290
810.601228	59.334406	70.920295
810.001381	66.060216	70.925300
810.139198	58.315301	70.930305
809.086215	66.828934	70.935310
808.287427	65.974497	70.940314
807.798054	54.893230	70.945319
806.913060	59.822546	70.950324
806.235818	58.997652	70.955329
805.618223	73.483275	70.960334
804.953947	61.056320	70.965338
804.665481	64.484076	70.970343
803.439104	53.348208	70.975348
802.895846	57.191821	70.980353
802.620741	57.687491	70.985358
801.789491	70.847787	70.990362
800.708914	53.287904	70.995367
799.944748	61.847039	71.000372
799.833475	51.431002	71.005377
799.156987	63.729307	71.010382
798.523374	51.239136	71.015386
797.458442	52.653699	71.020391
796.689573	59.097325	71.025396
796.370213	55.596180	71.030401
795.745515	64.226162	71.035406
794.624272	64.478019	71.040410
794.247707	63.614741	71.045415
793.814608	56.951002	71.050420
793.569686	62.413970	71.055425
792.142592	64.486985	71.060430
791.787799	59.690500	71.065434
791.522764	52.377126	71.070439
790.508236	60.927220	71.075444
789.383930	61.559610	71.080449
788.587205	63.931276	71.085454
788.141749	61.188208	71.090458
788.152476	60.588147	71.095463
787.774711	63.422992	71.100468
786.770392	55.929226	71.105473
786.025615	61.183161	71.110478
785.303309	58.346958	71.115482
784.655195	61.746795	71.120487
783.445206	64.983741	71.125492
783.193117	59.087554	71.130497
782.373751	64.304476	71.135502
781.161256	68.278255	71.140506
780.620664	57.711345	71.145511
780.272180	61.318963	71.150516
780.410622	56.289446	71.155521
779.715208	64.039712	71.160526
778.619899	64.741608	71.165530
778.295954	60.835921	71.170535
776.979727	60.147419	71.175540
776.169396	51.112077	71.180545
775.467087	60.074531	71.185550
774.904145	54.365012	71.190554
774.919413	59.857533	71.195559
773.959692	67.730290	71.200564
773.403606	56.585534	71.205569
772.675128	60.731441	71.210574
771.949881	62.457805	71.215578
771.461799	58.269161	71.220583
770.396735	61.437316	71.225588
770.121823	58.030025	71.230593
769.226156	65.905203	71.235598
769.003528	65.457397	71.240602
767.774608	57.425377	71.245607
767.007392	59.760814	71.250612
767.180606	55.779160	71.255617
766.002036	62.306922	71.260622
764.834380	64.669820	71.265626
764.529922	59.089475	71.270631
763.712543	67.024735	71.275636
763.515856	65.591942	71.280641
763.157739	68.414202	71.285646
762.096310	66.791031	71.290650
761.970655	63.383639	71.295655
760.701081	69.473307	71.300660
760.038836	64.186444	71.305665
759.240664	65.918111	71.310670
758.602453	62.530794	71.315674
757.921019	62.856172	71.320679
756.942385	73.617752	71.325684
756.763514	57.560711	71.330689
756.637166	71.892459	71.335694
755.676503	71.499037	71.340698
754.968976	63.194806	71.345703
754.242276	67.882906	71.350708
753.312339	70.384593	71.355713
752.281628	63.724512	71.360718
751.707936	63.946012	71.365722
751.742499	59.349340	71.370727
750.917433	61.131020	71.375732
750.426400	53.495656	71.380737
749.147391	63.538643	71.385742
748.591989	58.307321	71.390746
748.356678	58.593237	71.395751
747.357315	61.326746	71.400756
746.751361	52.391351	71.405761
745.897516	63.229258	71.410766
745.542596	58.188377	71.415770
745.192124	52.586976	71.420775
743.993051	61.431382	71.425780
743.543955	59.478951	71.430785
743.032203	54.860422	71.435790
742.346573	57.955581	71.440794
741.516080	50.747985	71.445799
740.779026	60.111786	71.450804
740.994953	50.047379	71.455809
739.606477	58.062498	71.460814
738.747463	64.443217	71.465818
738.333060	58.134481	71.470823
737.472265	64.755179	71.475828
736.722940	55.683333	71.480833
736.106480	61.501902	71.485838
735.823794	55.769865	71.490842
735.207463	51.516488	71.495847
733.958268	56.134787	71.500852
733.584671	57.202800	71.505857
733.001818	60.303680	71.510862
732.634344	55.802538	71.515866
731.456722	64.430649	71.520871
730.689133	63.315806	71.525876
730.325455	58.014550	71.530881
729.746296	66.657795	71.535886
729.072281	64.607125	71.540890
728.340068	65.501984	71.545895
727.597290	67.585963	71.550900
727.185239	51.588127	71.555905
726.103822	55.347100	71.560910
725.417988	57.642786	71.565914
725.142604	56.940032	71.570919
724.390587	65.637599	71.575924
724.061632	52.222184	71.580929
722.810929	56.807612	71.585934
722.387676	56.569938	71.590938
722.131713	57.332225	71.595943
721.456210	66.239963	71.600948
720.754805	62.515788	71.605953
720.071205	62.702750	71.610958
718.734627	65.284942	71.615962
717.998712	57.049902	71.620967
717.529268	65.057523	71.625972
717.465820	59.484556	71.630977
716.847992	58.859963	71.635982
715.547150	65.400900	71.640986
715.213255	55.797741	71.645991
714.498894	61.871591	71.650996
713.847162	60.758813	71.656001
712.762672	59.451569	71.661006
712.406521	57.642044	71.666010
712.220617	56.037231	71.671015
711.321481	67.885293	71.676020
710.416534	57.668135	71.681025
709.735097	58.360954	71.686030
709.316308	57.594296	71.691034
708.505467	55.502334	71.696039
707.280294	64.850800	71.701044
707.106329	55.050300	71.706049
706.530165	56.831798	71.711054
706.191280	58.528219	71.716058
705.130649	52.041661	71.721063
703.923334	64.022354	71.726068
703.632374	56.105998	71.731073
703.088403	54.830992	71.736078
702.693203	56.645187	71.741082
702.379453	59.796278	71.746087
701.320100	63.769368	71.751092
700.929237	60.252811	71.756097
700.267622	55.686533	71.761102
699.090064	55.991550	71.766106
698.538446	52.745009	71.771111
697.787306	61.567017	71.776116
697.536703	64.157706	71.781121
696.542770	62.930671	71.786126
695.626823	60.882251	71.791130
695.436310	57.650770	71.796135
694.761490	65.721047	71.801140
693.771839	54.331523	71.806145
693.191963	54.412095	71.811150
692.597821	48.940956	71.816154
692.335164	47.578596	71.821159
691.348597	62.419415	71.826164
690.900869	52.481148	71.831169
689.969552	47.842690	71.836174
689.233217	55.299863	71.841178
688.538606	50.177451	71.846183
687.878289	65.964544	71.851188
687.210550	54.716168	71.856193
686.850778	52.317448	71.861198
686.463428	53.422349	71.866202
685.242946	54.726100	71.871207
684.491029	61.132362	71.876212
684.127356	59.715120	71.881217
684.034862	68.536368	71.886222
682.595656	65.372771	71.891226
682.062278	59.289566	71.896231
681.345033	53.938948	71.901236
681.126525	48.698174	71.906241
680.085809	55.554103	71.911246
679.198808	60.447506	71.916250
678.976819	53.075261	71.921255
677.921261	56.513171	71.926260
677.732285	54.694386	71.931265
677.036889	61.965278	71.936270
676.176190	69.021214	71.941274
675.692614	65.314417	71.946279
674.435304	62.057216	71.951284
674.291133	63.979687	71.956289
673.750132	63.322375	71.961294
672.891446	67.359726	71.966298
672.405083	62.953212	71.971303
671.307461	68.458885	71.976308
671.031361	56.656164	71.981313
670.295361	64.993226	71.986318
669.286022	55.303636	71.991322
669.066461	55.391511	71.996327
668.444009	57.164616	72.001332
667.410563	61.795909	72.006337
666.531893	65.301860	72.011342
666.140199	66.901039	72.016346
666.221956	63.615178	72.021351
664.620638	72.992005	72.026356
664.215026	64.817939	72.031361
663.505155	69.427688	72.036366
662.920865	56.634825	72.041370
662.128167	65.745730	72.046375
661.026381	70.277521	72.051380
660.799105	59.848428	72.056385
660.488263	68.614549	72.061390
660.064301	67.271562	72.066394
659.469009	60.058091	72.071399
658.339899	71.449195	72.076404
657.860390	54.268373	72.081409
656.906893	60.120109	72.086414
656.087062	64.711093	72.091418
655.805962	67.938994	72.096423
655.231767	65.828300	72.101428
654.467833	61.057550	72.106433
653.469255	63.639583	72.111438
653.007829	64.767320	72.116442
652.802563	55.582089	72.121447
651.428737	60.037340	72.126452
650.859715	56.290538	72.131457
650.354527	64.475742	72.136462
650.076553	61.750194	72.141466
649.155230	55.974762	72.146471
647.961243	57.148158	72.151476
648.083799	45.117985	72.156481
647.444047	68.308693	72.161486
646.073272	57.112328	72.166490
645.591569	56.901318	72.171495
645.189970	64.954915	72.176500
644.778148	60.106037	72.181505
643.911394	55.654435	72.186510
642.635723	60.907766	72.191514
642.260326	53.966799	72.196519
641.774071	65.611951	72.201524
641.393420	57.992158	72.206529
640.316733	56.846128	72.211534
639.714403	57.956876	72.216538
639.507021	61.884240	72.221543
638.528183	63.116429	72.226548
637.543882	59.057276	72.231553
636.900558	63.043005	72.236558
636.359247	55.671140	72.241562
635.942320	56.126327	72.246567
635.369972	62.455127	72.251572
634.770082	57.432768	72.256577
634.159034	60.680081	72.261582
633.378774	63.542753	72.266586
632.455409	56.092942	72.271591
631.452317	55.882941	72.276596
631.190245	53.810872	72.281601
630.981634	64.557120	72.286606
629.986568	54.669738	72.291610
629.216462	56.996210	72.296615
628.332986	53.343632	72.301620
628.083652	52.964745	72.306625
627.256607	51.466744	72.311630
626.212155	58.430518	72.316634
626.207170	51.985668	72.321639
625.682189	64.373415	72.326644
625.082066	57.301073	72.331649
623.952883	59.356711	72.336654
623.408155	54.771848	72.341658
622.971700	54.015902	72.346663
621.507427	61.420253	72.351668
621.335838	51.890625	72.356673
620.711668	61.532942	72.361678
619.997108	69.885527	72.366682
619.158706	63.448780	72.371687
618.399526	69.063015	72.376692
618.206226	54.168938	72.381697
617.693088	62.237140	72.386702
616.672275	58.183810	72.391706
616.164299	59.673775	72.396711
615.104024	62.350799	72.401716
614.795618	58.939402	72.406721
613.976235	60.764373	72.411726
613.119958	60.485273	72.416730
612.799537	54.301953	72.421735
612.189291	61.420530	72.426740
611.691876	55.574469	72.431745
610.375843	52.083804	72.436750
609.783763	65.019973	72.441754
609.647410	56.430898	72.446759
609.045823	65.262231	72.451764
607.968165	57.333952	72.456769
607.332617	62.091149	72.461774
606.751287	61.225809	72.466778
606.568611	51.243791	72.471783
605.039262	58.776780	72.476788
604.646950	56.640295	72.481793
604.067345	53.179040	72.486798
603.949941	59.086907	72.491802
603.190232	56.989994	72.496807
602.009206	62.584663	72.501812
601.577603	50.877683	72.506817
601.117239	46.959057	72.511822
599.903235	67.990903	72.516826
599.505996	60.999805	72.521831
598.850086	65.812286	72.526836
598.316806	56.374939	72.531841
597.332860	58.390117	72.536846
596.492866	63.217715	72.541850
596.495135	61.825800	72.546855
596.181498	62.701360	72.551860
595.048190	52.858084	72.556865
593.983659	60.998310	72.561870
593.482040	61.623105	72.566874
593.124353	55.204450	72.571879
592.008676	64.347871	72.576884
591.763860	59.693185	72.581889
591.274967	68.197499	72.586894
590.697322	59.385377	72.591898
589.721618	60.101426	72.596903
588.942149	62.148706	72.601908
588.698510	61.888764	72.606913
587.435607	57.216408	72.611918
586.546866	64.420333	72.616922
586.609018	56.211237	72.621927
585.794358	61.009572	72.626932
584.812667	53.573801	72.631937
584.019440	62.933962	72.636942
583.373511	55.205036	72.641946
583.168543	64.238147	72.646951
582.380432	73.266343	72.651956
581.960822	58.291610	72.656961
581.229741	63.598606	72.661966
580.302643	58.642553	72.666970
579.053918	60.988478	72.671975
578.526699	59.762871	72.676980
578.855015	56.718450	72.681985
578.006960	59.123580	72.686990
577.231530	60.088440	72.691994
576.200707	56.853576	72.696999
575.237103	64.072577	72.702004
575.275152	57.825878	72.707009
574.608417	55.770940	72.712014
574.032014	57.524119	72.717018
573.423584	48.576563	72.722023
572.894731	60.964928	72.727028
571.766739	54.467083	72.732033
570.921822	57.120871	72.737038
570.103308	62.963758	72.742042
570.140726	57.671207	72.747047
569.178723	58.828202	72.752052
568.064985	62.862040	72.757057
567.646898	62.921611	72.762062
566.906885	67.072560	72.767066
567.041296	55.480464	72.772071
566.101573	66.097122	72.777076
565.124778	56.396095	72.782081
564.603066	58.011258	72.787086
564.023427	58.561750	72.792090
563.112535	53.905898	72.797095
562.173554	58.504840	72.802100
561.824315	50.515795	72.807105
561.433095	53.081574	72.812110
560.782134	59.309363	72.817114
559.867461	56.713595	72.822119
559.249667	63.284608	72.827124
558.909929	52.015594	72.832129
557.716657	61.940926	72.837134
556.859849	59.301252	72.842138
556.476464	48.781930	72.847143
555.960730	61.131937	72.852148
555.814282	53.116909	72.857153
554.717647	54.844121	72.862158
553.971022	62.949509	72.867162
553.366453	53.223912	72.872167
552.303752	57.850441	72.877172
551.768433	51.781777	72.882177
551.162616	50.131882	72.887182
550.894267	62.737386	72.892186
550.532865	43.612369	72.897191
549.263254	65.681242	72.902196
548.697380	57.810270	72.907201
548.338542	53.315674	72.912206
547.246788	60.075698	72.917210
546.297997	45.160025	72.922215
545.837545	66.332084	72.927220
545.855280	53.840791	72.932225
545.126621	53.303275	72.937230
543.871057	61.565400	72.942234
543.538754	51.427449	72.947239
542.729774	60.345429	72.952244
541.950106	42.127529	72.957249
541.063393	51.641349	72.962254
540.687335	59.697191	72.967258
540.396767	54.185638	72.972263
539.038388	57.924132	72.977268
538.502539	56.438137	72.982273
538.064199	57.715180	72.987278
537.501213	60.344585	72.992282
537.233793	56.778441	72.997287
536.124091	63.727408	73.002292
535.530178	58.950128	73.007297
534.746043	59.900617	73.012302
534.018750	54.915922	73.017306
533.079561	56.433569	73.022311
532.502625	65.426566	73.027316
532.212808	61.271060	73.032321
531.888914	63.107039	73.037326
530.758996	60.045669	73.042330
530.155725	54.678529	73.047335
529.437100	60.035591	73.052340
528.987831	60.647332	73.057345
528.483722	61.704617	73.062350
527.267183	59.177432	73.067354
527.099288	59.036320	73.072359
526.569927	65.060252	73.077364
525.449666	54.834894	73.082369
524.350672	58.040084	73.087374
524.053929	60.704364	73.092378
523.740726	59.939847	73.097383
523.490684	60.920404	73.102388
522.199836	48.938701	73.107393
521.711269	53.622044	73.112398
520.978545	59.438664	73.117402
520.282303	54.390682	73.122407
519.338522	58.075778	73.127412
518.917458	48.071817	73.132417
518.652131	54.957284	73.137422
517.652857	60.098847	73.142426
517.043450	56.718053	73.147431
516.433099	58.471919	73.152436
515.753434	56.710791	73.157441
514.666187	58.270946	73.162446
513.851452	45.331922	73.167450
513.810372	56.579754	73.172455
513.243977	62.057656	73.177460
512.596610	47.152344	73.182465
511.469190	55.349918	73.187470
511.052570	55.917038	73.192474
510.561502	57.049519	73.197479
509.429385	55.123906	73.202484
508.828337	55.166892	73.207489
508.304749	56.250936	73.212494
507.811368	59.668769	73.217498
507.325307	53.232731	73.222503
506.485007	66.763521	73.227508
505.921331	60.767190	73.232513
505.612592	58.234218	73.237518
504.359640	58.158674	73.242522
503.779171	52.955068	73.247527
503.194193	52.118719	73.252532
502.595562	54.708075	73.257537
501.472455	58.964202	73.262542
500.674922	63.245751	73.267546
500.500433	58.344915	73.272551
499.968199	62.711946	73.277556
499.452798	58.841528	73.282561
498.736243	58.839833	73.287566
497.738644	64.132523	73.292570
497.065908	58.181950	73.297575
496.061544	65.109425	73.302580
495.869424	57.333487	73.307585
495.185684	59.436510	73.312590
494.816133	60.287871	73.317594
494.033234	56.021666	73.322599
493.057709	59.984637	73.327604
493.026699	53.515555	73.332609
491.610664	62.705266	73.337614
490.482183	64.142690	73.342618
490.396059	53.624925	73.347623
489.712447	60.507626	73.352628
489.657518	47.119603	73.357633
488.937757	58.220056	73.362638
487.680329	62.693122	73.367642
487.339840	55.303511	73.372647
486.792271	60.784726	73.377652
485.664360	58.953070	73.382657
484.991582	59.321295	73.387662
484.526094	63.764431	73.392666
484.194898	57.105039	73.397671
483.302138	66.482652	73.402676
482.597076	54.128558	73.407681
482.164041	63.669493	73.412686
481.420392	60.466205	73.417690
480.521605	55.575072	73.422695
479.397548	56.614407	73.427700
479.192460	57.423807	73.432705
478.562486	57.107134	73.437710
478.313348	61.776008	73.442714
477.343174	55.335077	73.447719
476.289866	62.658280	73.452724
476.296627	51.986954	73.457729
475.660485	63.501446	73.462734
474.528221	69.638755	73.467738
474.255077	60.136360	73.472743
473.288475	61.891782	73.477748
473.019876	61.536479	73.482753
471.702329	57.448473	73.487758
470.945198	61.196898	73.492762
471.117090	59.256004	73.497767
470.427865	66.158528	73.502772
469.268749	56.328892	73.507777
468.675072	54.104656	73.512782
468.185197	63.523759	73.517786
467.808630	54.156111	73.522791
466.709126	57.607409	73.527796
466.193087	52.431398	73.532801
465.863752	59.047945	73.537806
464.394987	64.720037	73.542810
464.168070	59.185743	73.547815
463.394284	66.038658	73.552820
462.991714	56.637306	73.557825
461.863961	58.563476	73.562830
460.994137	61.768463	73.567834
460.597649	56.723220	73.572839
460.524165	61.605389	73.577844
460.047678	66.811941	73.582849
459.079219	57.972222	73.587854
457.895642	58.229425	73.592858
457.842565	48.220487	73.597863
456.616443	51.313489	73.602868
455.955902	58.015903	73.607873
455.539738	50.751894	73.612878
454.843007	59.283011	73.617882
454.644112	50.765425	73.622887
453.547618	58.448745	73.627892
452.909197	55.083629	73.632897
452.614931	62.856795	73.637902
451.401379	60.535752	73.642906
450.929349	54.106955	73.647911
449.824499	63.400085	73.652916
449.810675	60.493721	73.657921
449.217932	68.077890	73.662926
448.101816	63.642425	73.667930
448.096061	60.838854	73.672935
446.958938	67.289180	73.677940
446.090854	56.905429	73.682945
445.377554	56.097417	73.687950
444.700781	70.218758	73.692954
444.701621	58.655828	73.697959
443.547181	60.567333	73.702964
442.913857	52.016442	73.707969
442.300784	48.535331	73.712974
442.047708	59.269727	73.717978
441.417871	45.445010	73.722983
440.273866	56.244041	73.727988
439.648822	46.264708	73.732993
439.242715	52.191745	73.737998
437.849374	58.663958	73.743002
437.625718	53.185920	73.748007
436.665299	55.829761	73.753012
436.273262	51.545477	73.758017
435.949418	59.810626	73.763022
435.270363	54.039275	73.768026
434.237171	56.030819	73.773031
433.763921	60.169270	73.778036
433.216735	60.465466	73.783041
431.984377	57.319537	73.788046
431.296143	51.926539	73.793050
431.241935	44.880849	73.798055
430.635292	61.321722	73.803060
430.187577	47.743962	73.808065
429.158090	55.274692	73.813070
428.161661	59.567440	73.818074
427.882565	50.599014	73.823079
427.278882	50.251359	73.828084
426.185488	60.966643	73.833089
426.045981	50.045813	73.838094
425.458501	57.206522	73.843098
424.627977	45.591527	73.848103
423.527542	63.311104	73.853108
422.881913	58.754980	73.858113
422.852571	58.410458	73.863118
421.785048	54.632736	73.868122
421.368266	52.162718	73.873127
420.458747	60.439157	73.878132
420.154301	59.091370	73.883137
419.195769	62.761504	73.888142
418.282061	57.686693	73.893146
417.821681	54.734770	73.898151
417.267522	68.158499	73.903156
416.981725	58.284399	73.908161
415.990444	64.773005	73.913166
415.154118	63.270246	73.918170
414.740946	55.360801	73.923175
413.499128	55.712455	73.928180
413.248876	51.153281	73.933185
412.613959	55.091985	73.938190
412.070356	64.877616	73.943194
411.539028	59.765553	73.948199
410.438797	62.546792	73.953204
409.842261	60.113293	73.958209
409.372829	61.060999	73.963214
408.577791	58.684351	73.968218
407.930648	63.925977	73.973223
407.313816	61.451557	73.978228
406.971000	56.662702	73.983233
406.275398	58.930061	73.988238
404.855926	61.142418	73.993242
404.465956	50.168450	73.998247
403.954844	53.907663	74.003252
403.698342	53.916290	74.008257
402.397343	60.287079	74.013262
401.984241	52.331897	74.018266
401.509860	57.121807	74.023271
401.033195	62.908706	74.028276
400.030764	43.335504	74.033281
399.430146	61.946859	74.038286
398.857016	57.396540	74.043290
398.587855	44.558319	74.048295
397.153198	53.881920	74.053300
396.369296	55.690266	74.058305
395.923257	52.070597	74.063310
395.759679	53.023199	74.068314
394.880720	52.225822	74.073319
393.873728	60.584027	74.078324
393.891772	48.832292	74.083329
392.594066	58.984050	74.088334
391.331071	51.064910	74.093338
391.474608	45.104194	74.098343
390.668058	56.633221	74.103348
390.107703	52.500337	74.108353
389.860140	50.093254	74.113358
388.976987	53.245192	74.118362
388.635665	45.031003	74.123367
387.772509	62.257055	74.128372
386.726508	48.470268	74.133377
386.099552	51.623971	74.138382
385.484384	52.941822	74.143386
385.283786	48.392089	74.148391
383.799243	53.420190	74.153396
383.444290	53.558042	74.158401
382.894821	46.531328	74.163406
382.091112	56.295315	74.168410
381.407832	47.479596	74.173415
380.680241	56.520261	74.178420
380.390346	43.116074	74.183425
380.103742	56.763675	74.188430
378.965929	58.962716	74.193434
378.309274	57.883929	74.198439
377.868644	60.944876	74.203444
376.919076	57.648272	74.208449
375.803767	56.593666	74.213454
375.154572	61.483968	74.218458
374.987463	54.270187	74.223463
374.474568	55.950212	74.228468
373.843926	53.686158	74.233473
373.069338	46.515540	74.238478
371.939150	55.732304	74.243482
371.786799	56.966967	74.248487
371.251178	52.439067	74.253492
370.286346	44.002518	74.258497
369.666409	52.653876	74.263502
368.870182	54.896274	74.268506
368.632720	47.100777	74.273511
367.229790	63.042467	74.278516
366.768972	58.553112	74.283521
366.590515	48.836969	74.288526
365.724897	55.218837	74.293530
364.610270	58.199504	74.298535
363.846575	55.549799	74.303540
363.631296	56.045444	74.308545
363.171836	48.285314	74.313550
362.958581	56.804079	74.318554
361.892284	56.815564	74.323559
361.248209	54.049034	74.328564
360.684079	52.126044	74.333569
359.842845	59.809732	74.338574
358.498572	54.773580	74.343578
358.711159	56.248146	74.348583
358.032100	58.463997	74.353588
357.306555	52.274307	74.358593
356.508628	47.346659	74.363598
355.779737	56.094226	74.368602
355.413717	47.240589	74.373607
354.063470	61.179068	74.378612
353.658435	53.544307	74.383617
353.390731	52.189098	74.388622
352.772987	51.474699	74.393626
351.935421	54.907965	74.398631
351.160571	54.485097	74.403636
350.635357	54.025613	74.408641
350.037395	47.993795	74.413646
348.961134	59.562648	74.418650
348.241510	53.097631	74.423655
347.822945	57.367729	74.428660
347.186762	58.759899	74.433665
346.814385	44.791703	74.438670
345.829090	57.770034	74.443674
344.986491	62.735309	74.448679
344.674895	52.767570	74.453684
343.972936	54.062988	74.458689
343.316816	57.358541	74.463694
342.493903	53.461462	74.468698
342.234389	47.121840	74.473703
341.221658	61.071206	74.478708
340.461171	51.297986	74.483713
339.893955	46.790899	74.488718
339.191367	50.309895	74.493722
339.026991	51.341474	74.498727
337.623195	55.509922	74.503732
337.349811	51.722411	74.508737
337.112238	54.033507	74.513742
336.112336	57.224563	74.518746
335.470538	49.963416	74.523751
334.794114	54.523753	74.528756
333.908688	55.504632	74.533761
332.634563	54.200962	74.538766
331.938761	53.653544	74.543770
331.878716	45.659479	74.548775
331.635577	53.954348	74.553780
331.384785	50.443933	74.558785
330.397112	51.182487	74.563790
329.554766	58.374356	74.568794
329.033428	48.473155	74.573799
327.753784	53.137484	74.578804
327.262944	58.622301	74.583809
326.885824	54.387700	74.588814
326.238978	59.769641	74.593818
325.120508	54.287530	74.598823
324.230133	59.167383	74.603828
324.144817	54.980907	74.608833
323.702477	48.583685	74.613838
322.874181	50.559972	74.618842
322.071862	50.135183	74.623847
321.465289	43.797245	74.628852
320.842905	56.492259	74.633857
320.169203	60.732049	74.638862
319.215807	57.693119	74.643866
319.100365	60.978227	74.648871
318.409164	56.028855	74.653876
317.471051	47.096069	74.658881
316.764364	50.844379	74.663886
315.987626	60.977819	74.668890
315.736183	52.339320	74.673895
315.157160	51.101526	74.678900
314.119152	54.391700	74.683905
313.579905	50.780592	74.688910
313.133007	51.341530	74.693914
312.002612	53.009567	74.698919
311.192002	59.086223	74.703924
310.830740	50.597686	74.708929
310.412101	50.226884	74.713934
309.448280	61.858259	74.718938
309.002647	50.670838	74.723943
307.909832	53.332665	74.728948
307.810860	47.684974	74.733953
307.204534	49.690554	74.738958
306.180827	60.962468	74.743962
305.801316	60.440355	74.748967
304.946997	57.678954	74.753972
304.521669	56.388290	74.758977
303.853808	56.826742	74.763982
302.815206	61.149908	74.768986
302.633391	51.726042	74.773991
301.505362	52.404970	74.778996
300.747457	58.764964	74.784001
300.604296	52.350038	74.789006
299.633779	58.223520	74.794010
299.009548	52.933906	74.799015
297.945809	48.605291	74.804020
297.455241	55.072496	74.809025
297.191717	53.708744	74.814030
296.556771	47.430526	74.819034
295.601952	49.264557	74.824039
295.070482	54.916698	74.829044
294.563115	44.984900	74.834049
293.321875	58.451874	74.839054
292.609250	54.149315	74.844058
292.718506	51.945584	74.849063
291.925422	53.807462	74.854068
291.466258	50.897950	74.859073
290.586406	47.558738	74.864078
289.692542	53.145621	74.869082
289.340443	53.025991	74.874087
288.231969	50.103248	74.879092
287.520517	46.525894	74.884097
286.857090	52.687910	74.889102
286.498709	49.784418	74.894106
286.614457	56.205477	74.899111
285.422511	56.661211	74.904116
284.661250	55.928696	74.909121
283.584026	56.198996	74.914126
282.587360	55.089258	74.919130
282.183119	58.891887	74.924135
281.524811	59.800326	74.929140
281.412919	65.139614	74.934145
280.828420	51.490657	74.939150
279.605186	60.030008	74.944154
279.357102	47.636304	74.949159
278.827274	60.747081	74.954164
278.041862	47.415567	74.959169
276.934933	52.142283	74.964174
276.253507	49.949427	74.969178
276.205573	53.192237	74.974183
275.094880	55.027461	74.979188
274.397004	60.535814	74.984193
273.873916	57.306911	74.989198
273.449555	68.242067	74.994202
272.922365	47.841013	74.999207
271.718981	55.959315	75.004212
271.451860	56.428535	75.009217
271.040600	62.299644	75.014222
269.720910	59.530411	75.019226
269.321180	50.401471	75.024231
268.327643	57.021366	75.029236
267.900327	61.379601	75.034241
266.901262	53.000589	75.039246
265.931812	63.779753	75.044250
265.939672	48.971982	75.049255
265.140896	60.928724	75.054260
265.048327	61.631901	75.059265
264.443328	55.762075	75.064270
263.395065	57.946896	75.069274
262.860719	49.681491	75.074279
262.027230	58.862055	75.079284
261.092288	58.034223	75.084289
260.869458	60.366630	75.089294
259.825624	53.421880	75.094298
259.761979	49.700307	75.099303
258.588965	56.301497	75.104308
258.002523	54.366318	75.109313
257.298319	49.898428	75.114318
256.781173	62.387452	75.119322
255.957915	47.507123	75.124327
254.811450	59.479848	75.129332
254.838284	55.314929	75.134337
254.570499	60.532402	75.139342
253.465498	68.786426	75.144346
252.831419	52.891940	75.149351
252.067024	65.805138	75.154356
251.984857	54.454157	75.159361
250.900010	58.054591	75.164366
250.103931	67.290702	75.169370
249.851856	47.487630	75.174375
248.532418	65.579615	75.179380
247.974537	53.672092	75.184385
247.907672	58.531122	75.189390
246.928087	57.792410	75.194394
245.991758	55.532950	75.199399
244.985418	53.500688	75.204404
244.700181	56.879084	75.209409
244.450597	57.936863	75.214414
243.665999	52.295935	75.219418
242.657941	40.584741	75.224423
242.003853	64.933617	75.229428
241.293404	54.054916	75.234433
240.995932	51.364073	75.239438
240.075404	62.154370	75.244442
239.439862	54.728255	75.249447
238.931320	64.129853	75.254452
238.484198	56.787250	75.259457
237.654574	57.879117	75.264462
236.720354	59.907005	75.269466
236.440850	55.855559	75.274471
235.955421	52.410934	75.279476
234.970441	52.592438	75.284481
234.476479	65.776353	75.289486
233.431963	62.638439	75.294490
233.065643	49.825200	75.299495
231.919357	56.896797	75.304500
231.462022	58.910190	75.309505
231.010194	59.967084	75.314510
230.304891	62.303842	75.319514
229.924245	56.439273	75.324519
228.949043	62.797645	75.329524
228.314874	52.140180	75.334529
227.874262	50.989159	75.339534
226.805711	62.192551	75.344538
226.191411	57.139492	75.349543
225.471699	61.653138	75.354548
225.559978	62.839999	75.359553
224.599944	63.493766	75.364558
223.799236	66.440234	75.369562
223.181602	60.304353	75.374567
222.248579	47.133583	75.379572
221.216124	54.172851	75.384577
220.774678	56.781370	75.389582
220.107532	64.151927	75.394586
220.140750	58.918407	75.399591
219.476565	60.575264	75.404596
218.562341	62.033853	75.409601
218.082850	61.997613	75.414606
216.996503	54.747427	75.419610
216.439585	48.966148	75.424615
215.435624	53.510902	75.429620
215.051985	55.938324	75.434625
214.710711	55.708171	75.439630
213.525942	67.177670	75.444634
212.825915	57.967289	75.449639
211.976663	58.272250	75.454644
211.968767	61.182256	75.459649
211.753029	55.351333	75.464654
210.757209	45.153634	75.469658
210.217011	49.764825	75.474663
209.358709	60.114708	75.479668
208.300766	59.159845	75.484673
207.736513	54.702782	75.489678
207.120576	63.337764	75.494682
206.909642	58.852775	75.499687
205.524537	61.403535	75.504692
204.931246	50.507757	75.509697
204.587044	53.523398	75.514702
203.987778	61.531257	75.519706
203.620817	53.504116	75.524711
202.363138	59.920130	75.529716
201.563423	59.100731	75.534721
201.468572	53.480776	75.539726
200.666365	55.214827	75.544730
199.508193	57.335190	75.549735
198.933870	55.885366	75.554740
198.620685	52.534722	75.559745
198.690681	49.402126	75.564750
197.315157	60.943028	75.569754
196.570947	52.361010	75.574759
195.865912	55.795278	75.579764
195.485795	55.430971	75.584769
194.843528	51.133001	75.589774
193.777854	59.604698	75.594778
193.421570	50.208659	75.599783
192.538942	56.973327	75.604788
192.076394	53.551872	75.609793
191.553355	53.196153	75.614798
190.622112	58.582447	75.619802
190.426069	50.032914	75.624807
189.229665	58.536485	75.629812
188.764776	56.219256	75.634817
188.296331	48.219335	75.639822
186.881813	57.484635	75.644826
186.278992	47.620121	75.649831
185.741990	58.611073	75.654836
185.443608	50.104659	75.659841
185.199842	59.736869	75.664846
183.943664	53.067272	75.669850
183.478183	47.984203	75.674855
182.728981	56.924272	75.679860
182.454184	55.754715	75.684865
181.391852	55.620568	75.689870
180.771529	66.161188	75.694874
180.336924	47.530506	75.699879
178.932496	57.628398	75.704884
178.564116	54.316516	75.709889
178.332754	51.324990	75.714894
177.419481	59.151090	75.719898
177.313598	53.047201	75.724903
176.090138	52.281157	75.729908
175.461343	62.160814	75.734913
175.015668	57.870938	75.739918
174.095664	58.704421	75.744922
173.356768	54.570089	75.749927
172.802652	54.660868	75.754932
171.949699	52.345572	75.759937
171.725947	51.372883	75.764942
171.011960	58.727258	75.769946
170.269568	58.684045	75.774951
169.776191	60.263228	75.779956
168.899514	58.246600	75.784961
167.759575	52.840531	75.789966
167.243816	50.209722	75.794970
167.046817	41.930005	75.799975
166.342684	55.303528	75.804980
165.749121	54.927516	75.809985
165.169138	37.669878	75.814990
164.098374	52.979960	75.819994
163.993068	43.558122	75.824999
162.766344	49.152364	75.830004
162.056908	53.372653	75.835009
161.776335	52.407444	75.840014
160.960077	52.417007	75.845018
160.136725	52.112316	75.850023
159.233893	60.296298	75.855028
158.558820	44.463588	75.860033
158.921156	52.275601	75.865038
157.992924	48.521534	75.870042
157.021019	43.293691	75.875047
156.526936	55.856310	75.880052
155.574338	50.913966	75.885057
154.572272	45.897510	75.890062
153.640019	54.433105	75.895066
153.715460	49.162899	75.900071
153.032362	62.753849	75.905076
152.980781	58.049505	75.910081
152.204667	52.669030	75.915086
151.006154	53.814993	75.920090
150.648362	56.717690	75.925095
149.501743	48.138334	75.930100
149.121938	56.109641	75.935105
148.569502	59.956408	75.940110
147.822948	63.949233	75.945114
147.214675	57.693615	75.950119
146.293127	56.237651	75.955124
145.593176	56.058372	75.960129
145.349304	46.277005	75.965134
144.175066	48.865146	75.970138
143.537209	49.330396	75.975143
142.713166	62.533810	75.980148
142.802194	52.658376	75.985153
142.055007	49.048919	75.990158
141.006977	54.791306	75.995162
140.553282	55.446395	76.000167
139.965467	58.833608	76.005172
138.900887	56.466902	76.010177
138.426343	46.903652	76.015182
137.445051	65.954162	76.020186
137.297489	46.793626	76.025191
137.159030	60.578453	76.030196
135.961989	51.089367	76.035201
134.981977	52.238354	76.040206
134.449022	61.093504	76.045210
134.243270	52.621219	76.050215
132.876164	54.867954	76.055220
132.028725	55.653616	76.060225
132.195288	59.887240	76.065230
131.590533	58.249898	76.070234
130.915585	53.510885	76.075239
129.670429	54.284252	76.080244
129.237735	53.923606	76.085249
128.883445	58.987720	76.090254
127.584682	64.762199	76.095258
127.187198	63.948092	76.100263
126.452516	62.430809	76.105268
126.210290	52.668102	76.110273
125.244227	50.008160	76.115278
124.439774	61.984757	76.120282
124.231511	47.503193	76.125287
123.652117	51.767415	76.130292
122.755107	53.961296	76.135297
122.274560	54.811478	76.140302
121.595793	53.469785	76.145306
120.322393	46.749357	76.150311
119.592107	59.535711	76.155316
119.260653	55.861566	76.160321
118.998904	54.794015	76.165326
117.846672	58.823130	76.170330
117.359067	47.029034	76.175335
116.431251	49.232558	76.180340
116.139318	57.014821	76.185345
115.953558	50.267670	76.190350
114.815942	49.407549	76.195354
114.198815	54.338521	76.200359
113.619102	57.921564	76.205364
112.443361	60.749654	76.210369
111.966841	50.634798	76.215374
111.255590	53.093957	76.220378
111.123896	50.517053	76.225383
110.012670	55.231906	76.230388
109.192833	53.766050	76.235393
108.611412	51.361762	76.240398
108.058016	63.063379	76.245402
107.832573	46.368971	76.250407
106.729647	53.305972	76.255412
106.124778	56.934025	76.260417
105.799526	46.374020	76.265422
104.660387	55.330534	76.270426
103.972040	57.573159	76.275431
103.450542	52.943732	76.280436
102.648001	53.613438	76.285441
102.436814	54.680877	76.290446
101.503212	51.052266	76.295450
100.919454	47.322155	76.300455
100.207068	50.360230	76.305460
99.229297	58.348020	76.310465
98.578075	46.188935	76.315470
97.668185	58.316382	76.320474
97.489862	55.095639	76.325479
96.976767	61.132807	76.330484
97.024739	53.170430	76.335489
95.630767	58.584789	76.340494
94.570023	54.631101	76.345498
94.598092	53.462158	76.350503
93.779868	54.613755	76.355508
92.899889	48.519742	76.360513
92.373881	44.641658	76.365518
91.440236	47.333391	76.370522
90.839815	57.851921	76.375527
90.071803	62.876340	76.380532
89.628608	54.030336	76.385537
89.251466	44.694422	76.390542
88.138307	56.302349	76.395546
87.357478	48.804834	76.400551
86.827601	48.361919	76.405556
86.076674	48.436785	76.410561
86.035347	44.216510	76.415566
84.938976	51.329089	76.420570
84.342612	37.302072	76.425575
83.643162	46.691533	76.430580
83.309850	52.114997	76.435585
82.518300	44.921966	76.440590
81.437829	41.510742	76.445594
81.309788	49.424566	76.450599
80.439836	54.082043	76.455604
79.626066	47.387710	76.460609
79.331753	50.288178	76.465614
78.916439	54.575135	76.470618
77.975365	41.620192	76.475623
76.760025	49.601703	76.480628
76.370027	40.130652	76.485633
76.080646	49.092046	76.490638
74.649127	49.030995	76.495642
74.264152	45.482086	76.500647
73.627370	48.511268	76.505652
73.351941	49.864913	76.510657
72.299672	41.947066	76.515662
71.403326	53.492045	76.520666
71.130203	40.295001	76.525671
70.684612	53.614702	76.530676
69.818785	54.586240	76.535681
69.305000	49.536130	76.540686
68.385045	51.399379	76.545690
68.266204	50.309050	76.550695
67.321126	54.598468	76.555700
66.435558	51.093099	76.560705
66.301484	41.123938	76.565710
65.170368	53.185734	76.570714
64.323172	43.189918	76.575719
63.708219	52.553299	76.580724
63.158874	42.415382	76.585729
62.752496	36.925538	76.590734
61.531529	48.725694	76.595738
61.170362	42.350291	76.600743
60.712613	44.639737	76.605748
60.296972	44.593348	76.610753
59.288728	47.566640	76.615758
58.462307	49.173709	76.620762
58.070493	49.911986	76.625767
57.419762	50.838196	76.630772
56.377725	49.732633	76.635777
55.479991	40.186420	76.640782
54.988305	53.363662	76.645786
54.885203	55.486184	76.650791
54.087267	45.933518	76.655796
53.057935	42.826386	76.660801
52.505005	46.789938	76.665806
51.755999	50.392097	76.670810
51.580890	49.768050	76.675815
50.511323	47.425835	76.680820
49.846825	43.454727	76.685825
49.763086	42.057610	76.690830
48.538900	57.683919	76.695834
47.889191	53.445526	76.700839
47.166151	60.761948	76.705844
46.747774	42.800509	76.710849
46.315569	42.105491	76.715854
45.186710	49.772034	76.720858
44.801266	49.520563	76.725863
44.191516	51.135669	76.730868
43.405774	44.099420	76.735873
42.471385	45.979171	76.740878
41.414171	48.383122	76.745882
41.539359	41.382985	76.750887
41.171799	55.838251	76.755892
40.345874	44.572779	76.760897
39.628410	47.190639	76.765902
38.701276	56.553339	76.770906
38.245139	46.684413	76.775911
37.203279	51.684697	76.780916
36.711373	41.942901	76.785921
36.206582	41.894961	76.790926
35.455393	57.545205	76.795930
34.734581	44.381700	76.800935
34.015375	53.370630	76.805940
33.365649	48.036281	76.810945
32.979029	43.473678	76.815950
32.313814	51.783805	76.820954
31.498393	36.976464	76.825959
30.396036	52.608580	76.830964
29.910307	49.522014	76.835969
29.772033	47.204782	76.840974
29.120736	49.197094	76.845978
28.494719	38.699261	76.850983
27.776966	54.139171	76.855988
26.832995	54.727374	76.860993
25.961182	50.453441	76.865998
25.432186	51.503750	76.871002
25.011080	51.300545	76.876007
24.069757	52.821868	76.881012
23.241775	48.522024	76.886017
22.645599	53.068057	76.891022
21.965598	51.907937	76.896026
21.876925	50.637762	76.901031
21.431769	43.881526	76.906036
20.239807	38.111680	76.911041
19.884543	49.996165	76.916046
18.923207	42.573193	76.921050
18.094535	39.369429	76.926055
17.339235	49.113155	76.931060
16.829476	61.618362	76.936065
16.558282	43.214002	76.941070
15.926120	48.260928	76.946074
15.214505	50.816362	76.951079
14.612510	45.800833	76.956084
13.770346	43.417646	76.961089
12.851690	42.664583	76.966094
12.094721	56.210553	76.971098
11.716193	52.998089	76.976103
11.041630	55.970234	76.981108
10.118244	53.811306	76.986113
9.444520	49.381216	76.991118
9.007973	54.218762	76.996122
8.763574	44.390200	77.001127
7.852755	50.246370	77.006132
6.909983	46.775378	77.011137
6.363533	42.438536	77.016142
5.735766	51.958507	77.021147
5.326167	50.387851	77.026151
4.448790	53.527952	77.031156
3.989936	49.185026	77.036161