Mon Mar 08 17:50:14 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.583643	96.954620	0.000000
0.118382	95.521053	0.005005
-0.768650	47.423987	0.010010
-2.343709	-0.271437	0.015014
-6.944583	-3.896367	0.020019
-11.868581	-11.661203	0.025024
-17.257349	-9.177583	0.030029
-21.751661	-2.681448	0.035034
-25.625317	-5.034659	0.040038
-29.234568	-2.387045	0.045043
-32.670151	-4.723398	0.050048
-36.348791	-3.531242	0.055053
-40.261708	-1.027552	0.060058
-43.897932	-4.814188	0.065062
-47.712392	-0.049117	0.070067
-50.776630	-7.829876	0.075072
-55.222998	5.146130	0.080077
-58.738051	-3.496237	0.085082
-62.699105	-13.027782	0.090086
-66.732054	0.576128	0.095091
-70.010308	-1.602350	0.100096
-74.090997	-0.070031	0.105101
-77.768941	1.825384	0.110106
-81.382873	-2.229675	0.115110
-85.333617	4.358043	0.120115
-89.099787	-3.274404	0.125120
-93.010742	-0.133867	0.130125
-96.588198	-4.787644	0.135130
-100.184290	-11.754936	0.140134
-104.291943	-4.782619	0.145139
-107.516421	-14.570381	0.150144
-111.747942	-12.340588	0.155149
-115.365103	-16.221613	0.160154
-118.811345	-16.174990	0.165158
-123.496923	1.778212	0.170163
-127.266606	-6.232071	0.175168
-130.846019	0.864155	0.180173
-134.654500	-6.964887	0.185178
-138.202768	-1.330695	0.190182
-141.891570	5.011889	0.195187
-145.528785	-4.046079	0.200192
-149.301388	3.151964	0.205197
-152.919416	5.840583	0.210202
-156.704006	3.292025	0.215206
-160.735655	5.802239	0.220211
-164.118135	-5.491424	0.225216
-168.032667	8.918478	0.230221
-171.860225	-1.499919	0.235226
-175.660645	-1.321001	0.240230
-179.586946	11.808763	0.245235
-183.263716	-5.673052	0.250240
-187.219286	10.429157	0.255245
-190.579517	-4.083360	0.260250
-194.194425	2.972891	0.265254
-198.381913	2.858811	0.270259
-202.031112	-6.512537	0.275264
-205.597026	5.315554	0.280269
-208.920140	5.219654	0.285274
-212.817288	-5.905062	0.290278
-217.207301	9.755607	0.295283
-220.802097	0.951178	0.300288
-224.601687	-1.648492	0.305293
-228.552742	-0.308490	0.310298
-232.194323	3.368003	0.315302
-236.252387	4.045445	0.320307
-239.455433	-1.379065	0.325312
-243.368161	3.903450	0.330317
-247.012758	0.511117	0.335322
-250.549109	4.976646	0.340326
-254.890573	10.324462	0.345331
-258.555477	-1.058018	0.350336
-262.208875	5.848359	0.355341
-266.056103	-1.228399	0.360346
-269.978289	-2.479084	0.365350
-273.775189	6.509672	0.370355
-277.159028	5.408024	0.375360
-280.799334	3.079478	0.380365
-284.719602	8.180340	0.385370
-288.274001	2.305793	0.390374
-292.486492	7.875930	0.395379
-296.029852	-8.270833	0.400384
-299.791555	-2.416266	0.405389
-303.332261	9.595589	0.410394
-306.925614	8.346084	0.415398
-311.169981	10.412698	0.420403
-314.855864	1.351730	0.425408
-318.797130	10.403025	0.430413
-322.444330	9.255178	0.435418
-325.765633	-0.095783	0.440422
-329.965800	8.255710	0.445427
-333.740734	2.550480	0.450432
-337.824400	7.600244	0.455437
-341.614434	6.736999	0.460442
-344.948322	1.265718	0.465446
-349.011755	4.382122	0.470451
-352.193354	3.768673	0.475456
-356.331334	8.655256	0.480461
-359.717713	3.633912	0.485466
-363.626281	4.420161	0.490470
-367.735107	13.479364	0.495475
-371.020864	1.047804	0.500480
-374.850555	10.276908	0.505485
-378.956907	3.872479	0.510490
-382.530461	5.207649	0.515494
-386.536574	6.578777	0.520499
-390.158378	4.148100	0.525504
-393.933493	-2.298152	0.530509
-397.845984	3.547527	0.535514
-401.304208	7.344799	0.540518
-405.146057	5.725124	0.545523
-408.429500	-0.194080	0.550528
-412.398224	4.540992	0.555533
-416.485353	7.569831	0.560538
-420.244010	-0.597845	0.565542
-424.156543	6.515723	0.570547
-427.965503	-2.262057	0.575552
-431.544348	1.792632	0.580557
-435.148794	3.143851	0.585562
-439.200188	-2.791438	0.590566
-443.117640	6.522743	0.595571
-446.313472	2.813053	0.600576
-450.178051	-2.753091	0.605581
-453.991066	4.350938	0.610586
-457.340460	-0.173131	0.615590
-461.701454	13.411245	0.620595
-465.453130	10.134119	0.625600
-469.251913	13.500188	0.630605
-473.158504	7.737365	0.635610
-476.670646	3.228278	0.640614
-480.593638	4.291404	0.645619
-483.980830	-8.029162	0.650624
-487.976817	8.477324	0.655629
-491.621673	4.886721	0.660634
-495.174566	4.123036	0.665638
-499.318122	1.130904	0.670643
-502.925465	1.172271	0.675648
-506.849948	3.257518	0.680653
-510.390947	-2.648784	0.685658
-513.914387	-0.739543	0.690662
-517.760288	5.190304	0.695667
-521.128798	0.319306	0.700672
-525.803315	2.636349	0.705677
-529.466283	1.186996	0.710682
-533.175844	-1.716708	0.715686
-537.457338	10.334948	0.720691
-540.611077	7.585312	0.725696
-544.214269	9.209300	0.730701
-548.046591	-0.392427	0.735706
-551.884546	-0.063418	0.740710
-555.955172	1.789795	0.745715
-559.301878	-0.337645	0.750720
-563.247981	2.851834	0.755725
-566.654742	-2.208523	0.760730
-570.540065	-0.228773	0.765734
-574.660257	2.988535	0.770739
-578.196971	1.987431	0.775744
-582.248978	8.699339	0.780749
-585.810958	-0.190170	0.785754
-589.301991	-0.211407	0.790758
-593.258223	8.711820	0.795763
-596.800557	5.992805	0.800768
-600.608465	-1.521743	0.805773
-604.671574	-0.155338	0.810778
-608.437672	6.394242	0.815782
-612.199470	5.372381	0.820787
-615.800752	-0.189821	0.825792
-619.468462	4.544798	0.830797
-623.414466	7.940935	0.835802
-627.063008	-0.138336	0.840806
-630.973647	6.284565	0.845811
-634.570991	-0.776303	0.850816
-638.281551	7.331899	0.855821
-642.222304	7.317943	0.860826
-645.663494	3.805424	0.865830
-649.911405	7.331843	0.870835
-653.221590	-3.617814	0.875840
-657.249739	3.549284	0.880845
-660.995168	-5.427480	0.885850
-664.471757	-4.667189	0.890854
-668.277836	2.771939	0.895859
-672.142784	-5.559674	0.900864
-676.288483	-0.311786	0.905869
-679.833569	-7.603274	0.910874
-683.443738	-6.592958	0.915878
-687.732588	-3.920926	0.920883
-691.161501	-2.176338	0.925888
-694.773682	-0.077615	0.930893
-698.374587	3.425917	0.935898
-702.002677	-7.950663	0.940902
-706.364032	8.967766	0.945907
-709.889609	-2.172883	0.950912
-713.790779	4.735901	0.955917
-717.494064	7.744905	0.960922
-721.222831	-5.466850	0.965926
-725.108979	4.869331	0.970931
-728.186100	-3.096098	0.975936
-732.075976	-1.454395	0.980941
-736.148861	-4.608783	0.985946
-740.262083	-1.433307	0.990950
-744.020587	6.987058	0.995955
-747.417336	-2.278673	1.000960
-751.401923	8.137937	1.005965
-755.126724	2.641427	1.010970
-758.647468	-2.778883	1.015974
-762.897887	1.689550	1.020979
-766.443059	-5.483520	1.025984
-770.059008	5.553844	1.030989
-773.526248	-9.456296	1.035994
-777.242242	-2.884511	1.040998
-781.277534	6.373337	1.046003
-784.894130	-1.734436	1.051008
-788.919767	4.254523	1.056013
-792.971293	3.250879	1.061018
-796.460136	1.157538	1.066022
-800.485180	8.024761	1.071027
-803.557690	-4.162687	1.076032
-807.594564	5.092301	1.081037
-811.144741	3.729434	1.086042
-815.014583	2.058137	1.091046
-819.517738	1.557230	1.096051
-822.586094	-10.118354	1.101056
-826.460419	4.079517	1.106061
-829.998515	-0.137881	1.111066
-834.034246	6.213878	1.116070
-838.030604	6.825709	1.121075
-841.244515	-5.835804	1.126080
-845.247264	1.141462	1.131085
-848.979463	0.036404	1.136090
-852.570581	2.639763	1.141094
-856.819647	2.490957	1.146099
-860.420683	-0.295537	1.151104
-864.254499	0.657772	1.156109
-868.109297	6.722048	1.161114
-871.717701	-1.502007	1.166118
-875.629595	9.636439	1.171123
-878.874020	-1.725500	1.176128
-882.794381	1.829381	1.181133
-886.292628	5.523355	1.186138
-890.197892	2.416552	1.191142
-894.311662	2.990483	1.196147
-897.924031	-1.754237	1.201152
-901.627684	6.272829	1.206157
-905.365285	2.446982	1.211162
-909.172630	5.621148	1.216166
-912.661792	10.075354	1.221171
-916.977796	3.366384	1.226176
-920.626934	-3.252092	1.231181
-924.298187	-5.486378	1.236186
-927.932039	-2.002467	1.241190
-931.895716	3.601515	1.246195
-935.319116	-5.233896	1.251200
-939.173900	-2.014252	1.256205
-943.151877	-2.267750	1.261210
-946.576418	-2.811586	1.266214
-950.361027	1.950108	1.271219
-954.182356	-2.130343	1.276224
-958.374196	-0.872054	1.281229
-962.219520	9.815924	1.286234
-965.801632	2.418845	1.291238
-969.538598	11.485793	1.296243
-973.009021	1.049511	1.301248
-977.050996	4.250269	1.306253
-980.815388	6.592957	1.311258
-984.619574	5.983739	1.316262
-988.345182	9.660608	1.321267
-991.623682	-2.993505	1.326272
-995.971658	9.910044	1.331277
-999.608900	0.922855	1.336282
-1003.109199	-2.008832	1.341286
-1007.217317	2.888267	1.346291
-1010.811209	1.868578	1.351296
-1014.691296	0.588748	1.356301
-1018.312156	0.519527	1.361306
-1021.744781	-2.971718	1.366310
-1026.082539	3.337204	1.371315
-1029.822112	5.647617	1.376320
-1033.487996	6.189575	1.381325
-1037.104117	-0.240034	1.386330
-1040.524994	-1.249505	1.391334
-1044.394663	6.233489	1.396339
-1048.294734	1.453028	1.401344
-1052.568360	9.486337	1.406349
-1055.981884	11.380373	1.411354
-1059.748437	-0.150081	1.416358
-1063.532032	7.002217	1.421363
-1066.874543	-9.282609	1.426368
-1070.686860	3.932758	1.431373
-1074.787441	-2.904980	1.436378
-1078.459219	1.242796	1.441382
-1082.243865	-0.127879	1.446387
-1085.870769	-7.588553	1.451392
-1089.680217	-8.814903	1.456397
-1093.362391	-4.096181	1.461402
-1097.303944	-3.423293	1.466406
-1101.395019	10.770247	1.471411
-1104.977064	1.971515	1.476416
-1108.662352	2.340082	1.481421
-1112.521820	2.417986	1.486426
-1116.132015	5.078409	1.491430
-1119.776804	5.492553	1.496435
-1123.375257	0.425856	1.501440
-1127.406265	2.854008	1.506445
-1131.333436	13.809223	1.511450
-1134.904018	7.211638	1.516454
-1138.765897	8.512073	1.521459
-1142.381117	1.661456	1.526464
-1146.342362	15.019040	1.531469
-1150.216479	1.295133	1.536474
-1153.652599	3.694379	1.541478
-1157.502889	6.579355	1.546483
-1161.156582	-2.048552	1.551488
-1164.694469	-4.529290	1.556493
-1168.737378	-1.537786	1.561498
-1172.375133	-9.461767	1.566502
-1176.724858	5.812452	1.571507
-1180.242516	-5.953147	1.576512
-1183.724551	-3.355706	1.581517
-1187.600423	3.165017	1.586522
-1191.001275	-1.269313	1.591526
-1194.754326	4.556855	1.596531
-1198.894928	-6.096661	1.601536
-1202.904191	-3.712860	1.606541
-1206.430767	-3.279651	1.611546
-1209.677783	-8.728862	1.616550
-1214.053061	4.619382	1.621555
-1217.584372	6.616075	1.626560
-1221.478461	7.029273	1.631565
-1225.275893	7.237782	1.636570
-1228.771816	-3.736459	1.641574
-1232.636195	-6.428185	1.646579
-1236.336282	-19.318777	1.651584
-1240.548184	5.912118	1.656589
-1244.227125	11.234512	1.661594
-1247.654310	2.794417	1.666598
-1251.576205	-4.350703	1.671603
-1255.273674	-6.969757	1.676608
-1259.433317	2.106922	1.681613
-1262.944762	-0.931388	1.686618
-1266.288562	-1.085564	1.691622
-1270.189029	7.645314	1.696627
-1273.662016	3.982718	1.701632
-1277.627097	3.896457	1.706637
-1281.561667	8.871903	1.711642
-1285.466429	-3.146948	1.716646
-1289.616569	8.870762	1.721651
-1292.987999	5.437937	1.726656
-1296.547691	5.163824	1.731661
-1300.290959	0.975271	1.736666
-1304.034434	2.135604	1.741670
-1308.029447	5.078681	1.746675
-1311.605644	-1.159758	1.751680
-1315.809376	5.804722	1.756685
-1319.446529	3.475726	1.761690
-1322.757064	-0.994938	1.766694
-1326.385487	5.648820	1.771699
-1330.210345	1.180073	1.776704
-1334.132373	5.480261	1.781709
-1338.081397	-0.204885	1.786714
-1341.907292	-3.773034	1.791718
-1345.549930	7.017120	1.796723
-1349.355204	-5.558415	1.801728
-1352.958533	3.150255	1.806733
-1357.237702	7.375195	1.811738
-1360.666125	-11.487821	1.816742
-1364.393613	1.034759	1.821747
-1367.595347	-2.339965	1.826752
-1371.850020	9.301969	1.831757
-1375.950766	4.335013	1.836762
-1378.988880	8.796531	1.841766
-1383.155617	8.138782	1.846771
-1386.513990	9.436284	1.851776
-1390.849538	15.747090	1.856781
-1394.569473	6.042114	1.861786
-1398.245095	4.725465	1.866790
-1402.141603	0.355042	1.871795
-1405.945202	4.894999	1.876800
-1409.379973	2.560552	1.881805
-1413.377506	12.026267	1.886810
-1416.875545	1.349127	1.891814
-1420.624199	10.823888	1.896819
-1424.539747	1.128211	1.901824
-1428.459006	3.319798	1.906829
-1432.072831	-2.612810	1.911834
-1435.842812	-1.441713	1.916838
-1439.711918	10.359367	1.921843
-1443.038987	6.646861	1.926848
-1446.970424	11.167932	1.931853
-1450.992824	3.045811	1.936858
-1454.854554	4.387743	1.941862
-1458.551014	14.275239	1.946867
-1462.005777	5.570248	1.951872
-1466.037719	5.359404	1.956877
-1469.475150	10.801159	1.961882
-1472.907566	3.928118	1.966886
-1477.332084	17.223218	1.971891
-1480.859167	3.499533	1.976896
-1484.551373	2.045335	1.981901
-1488.819930	1.937076	1.986906
-1492.047254	8.209355	1.991910
-1496.032450	11.529637	1.996915
-1500.235389	0.680161	2.006912
-1500.539744	6.232536	2.016909
-1498.408243	5.705977	2.026906
-1495.721362	7.708321	2.036902
-1493.584151	-3.776826	2.046899
-1491.405113	2.899918	2.056896
-1489.703584	4.665339	2.066893
-1487.771910	3.150811	2.076890
-1485.727871	0.481471	2.086886
-1483.752520	0.990438	2.096883
-1481.886210	5.004696	2.106880
-1480.549849	0.787667	2.116877
-1478.303067	10.987196	2.126874
-1476.389621	6.955644	2.136870
-1474.405268	2.566956	2.146867
-1472.316222	9.884965	2.156864
-1470.537566	4.662394	2.166861
-1468.762896	7.949248	2.176858
-1467.221806	12.438749	2.186854
-1464.899300	6.803836	2.196851
-1463.123547	6.140070	2.206848
-1460.737460	6.466446	2.216845
-1459.275153	6.399181	2.226842
-1458.031213	9.992078	2.236838
-1455.318404	3.243117	2.246835
-1453.547799	2.073350	2.256832
-1451.751392	-0.437889	2.266829
-1449.880965	-0.707865	2.276826
-1448.029204	-0.633805	2.286822
-1446.179500	-2.267802	2.296819
-1444.101755	-0.213647	2.306816
-1442.437487	-3.047924	2.316813
-1440.500580	-2.850126	2.326810
-1438.428152	-2.328243	2.336806
-1436.603342	4.774745	2.346803
-1434.951603	1.610905	2.356800
-1432.971131	2.897503	2.366797
-1431.239492	2.851866	2.376794
-1429.141633	1.580772	2.386790
-1427.155527	-1.878173	2.396787
-1425.384044	1.102914	2.406784
-1423.655744	2.628841	2.416781
-1421.774923	1.858285	2.426778
-1420.086224	2.620043	2.436774
-1417.683450	-1.603490	2.446771
-1416.019712	0.556451	2.456768
-1414.144097	-3.101104	2.466765
-1412.332813	-2.946325	2.476762
-1410.516760	-6.325925	2.486758
-1408.382230	-6.646047	2.496755
-1406.639227	2.170557	2.506752
-1404.651657	0.692937	2.516749
-1402.842155	4.976880	2.526746
-1400.921177	4.694113	2.536742
-1399.126989	-1.812972	2.546739
-1396.966539	-0.945151	2.556736
-1395.305117	0.280457	2.566733
-1393.533180	-0.382644	2.576730
-1391.745423	4.233204	2.586726
-1389.792875	3.847499	2.596723
-1387.864875	-4.332549	2.606720
-1385.839454	-4.276768	2.616717
-1384.002635	-0.797696	2.626714
-1382.289430	9.872617	2.636710
-1380.434126	1.247902	2.646707
-1378.306275	6.966662	2.656704
-1376.540809	-0.563686	2.666701
-1374.731999	5.394044	2.676698
-1372.867801	0.508370	2.686694
-1370.660992	0.001451	2.696691
-1369.126197	1.285245	2.706688
-1367.255235	3.320472	2.716685
-1365.311756	5.088306	2.726682
-1363.389310	3.467991	2.736678
-1361.635631	0.726822	2.746675
-1359.939562	6.178413	2.756672
-1357.754820	5.368729	2.766669
-1355.863172	10.413233	2.776666
-1354.123272	5.579048	2.786662
-1351.990358	6.749736	2.796659
-1350.231629	2.689369	2.806656
-1348.376879	0.502020	2.816653
-1346.578119	-2.037937	2.826650
-1344.664466	0.364678	2.836646
-1342.857661	5.198566	2.846643
-1340.632990	7.661922	2.856640
-1339.066295	0.141313	2.866637
-1337.236273	0.364204	2.876634
-1335.168708	3.575858	2.886630
-1333.351129	2.037091	2.896627
-1331.573716	11.471930	2.906624
-1329.838754	6.112772	2.916621
-1327.541367	4.699306	2.926618
-1325.645862	2.164404	2.936614
-1324.178269	9.913610	2.946611
-1322.046612	6.464608	2.956608
-1320.393858	5.301175	2.966605
-1318.447386	1.215516	2.976602
-1316.408855	9.924899	2.986598
-1314.656007	7.014952	2.996595
-1312.709998	13.511294	3.006592
-1310.736899	5.802492	3.016589
-1308.968319	7.191009	3.026586
-1307.112681	8.248230	3.036582
-1305.279020	8.544773	3.046579
-1303.329852	6.823916	3.056576
-1301.497161	8.674275	3.066573
-1299.696949	11.055615	3.076570
-1297.335057	10.197106	3.086566
-1296.024739	10.705316	3.096563
-1294.077373	8.282135	3.106560
-1291.902889	10.158320	3.116557
-1290.068305	10.615777	3.126554
-1288.352638	7.353385	3.136550
-1286.689195	8.948218	3.146547
-1284.417799	5.492673	3.156544
-1282.678672	5.785418	3.166541
-1280.727894	3.382228	3.176538
-1279.054206	6.664872	3.186534
-1277.314143	1.998082	3.196531
-1275.074894	1.216067	3.206528
-1272.808292	4.127507	3.216525
-1271.611219	1.178652	3.226522
-1269.965642	0.944809	3.236518
-1267.553090	3.376587	3.246515
-1265.863933	2.985775	3.256512
-1263.776899	5.310185	3.266509
-1261.991718	3.274562	3.276506
-1260.173034	5.343507	3.286502
-1258.694862	4.334373	3.296499
-1256.350017	3.682315	3.306496
-1254.411540	4.702638	3.316493
-1252.475332	1.896021	3.326490
-1250.931598	7.698916	3.336486
-1248.687307	3.654068	3.346483
-1247.047267	0.084868	3.356480
-1245.145607	7.148884	3.366477
-1243.503692	-0.408968	3.376474
-1241.599404	6.411476	3.386470
-1239.280043	5.864565	3.396467
-1237.521425	8.050509	3.406464
-1235.803869	3.025776	3.416461
-1233.673614	5.220142	3.426458
-1232.255050	9.697842	3.436454
-1230.104929	9.913802	3.446451
-1228.368792	6.141343	3.456448
-1226.153108	3.400547	3.466445
-1224.347909	12.071573	3.476442
-1222.871859	5.175001	3.486438
-1221.105863	3.846677	3.496435
-1218.807144	2.246791	3.506432
-1216.986723	-1.013365	3.516429
-1215.058022	-2.531929	3.526426
-1213.356036	3.097249	3.536422
-1211.397227	4.801185	3.546419
-1209.302307	6.315976	3.556416
-1207.686692	2.755447	3.566413
-1205.708577	7.034678	3.576410
-1203.658839	2.796798	3.586406
-1202.077048	3.054782	3.596403
-1199.981657	-2.000386	3.606400
-1198.410512	-2.605946	3.616397
-1196.594193	-4.076512	3.626394
-1194.374086	-1.689649	3.636390
-1192.736046	-2.362750	3.646387
-1190.774710	0.880247	3.656384
-1188.655158	0.954296	3.666381
-1186.847832	-2.521632	3.676378
-1185.012997	-4.969347	3.686374
-1183.357227	9.130272	3.696371
-1181.472511	1.895180	3.706368
-1179.293771	-0.905976	3.716365
-1177.722043	-2.001080	3.726362
-1175.489935	4.659602	3.736358
-1173.963408	7.504828	3.746355
-1172.286030	-1.156005	3.756352
-1170.216945	-0.953865	3.766349
-1168.092548	0.843611	3.776346
-1166.190027	-3.755938	3.786342
-1164.384498	2.079339	3.796339
-1162.570053	5.420075	3.806336
-1160.756638	-3.050940	3.816333
-1158.881931	-3.139789	3.826330
-1157.232559	-3.203636	3.836326
-1155.095051	-2.642963	3.846323
-1152.874753	0.574423	3.856320
-1151.099529	-1.036373	3.866317
-1149.287584	-2.150945	3.876314
-1147.638411	3.156740	3.886310
-1146.074141	-7.983830	3.896307
-1143.706988	-5.072560	3.906304
-1141.884863	-6.814008	3.916301
-1140.018126	-9.033111	3.926298
-1137.947986	-1.080184	3.936294
-1136.447346	-2.220729	3.946291
-1134.675563	0.515811	3.956288
-1132.751707	-0.269291	3.966285
-1130.568219	-2.876953	3.976282
-1128.642251	-7.985478	3.986278
-1126.631831	-0.739815	3.996275
-1125.341836	0.357523	4.006272
-1123.082083	-0.512888	4.016269
-1121.434637	-1.820592	4.026266
-1119.589092	-1.960006	4.036262
-1117.682835	2.316588	4.046259
-1115.585429	6.112612	4.056256
-1113.744884	5.140331	4.066253
-1112.007384	0.537224	4.076250
-1109.989936	7.300210	4.086246
-1107.985444	0.805473	4.096243
-1106.310424	-0.501895	4.106240
-1104.686886	5.471495	4.116237
-1102.439554	5.687811	4.126234
-1100.706729	2.307546	4.136230
-1098.624338	9.765934	4.146227
-1096.844241	3.160262	4.156224
-1095.199150	7.166031	4.166221
-1093.048580	0.526360	4.176218
-1091.386885	5.069466	4.186214
-1089.390973	-1.393883	4.196211
-1087.522325	3.220328	4.206208
-1085.542871	-7.495581	4.216205
-1083.559510	-3.343397	4.226202
-1081.966836	-0.183432	4.236198
-1080.055624	5.998164	4.246195
-1078.112456	-2.029347	4.256192
-1076.091304	-0.047903	4.266189
-1074.487790	0.255639	4.276186
-1072.471967	-0.582019	4.286182
-1070.877532	2.565041	4.296179
-1068.795392	0.175748	4.306176
-1066.787918	-1.295296	4.316173
-1064.894975	-0.030691	4.326170
-1063.075559	-0.806924	4.336166
-1061.166608	0.695119	4.346163
-1059.422071	-1.261221	4.356160
-1057.502133	6.867393	4.366157
-1055.704525	2.682598	4.376154
-1053.729216	3.888249	4.386150
-1051.813733	4.252431	4.396147
-1050.245799	6.457970	4.406144
-1047.857948	7.610269	4.416141
-1046.156828	-1.510591	4.426138
-1044.628619	1.186035	4.436134
-1042.464967	2.890509	4.446131
-1040.702941	0.462445	4.456128
-1038.696250	5.739872	4.466125
-1036.768222	-2.788864	4.476122
-1034.710220	-0.702753	4.486118
-1032.885437	-4.064519	4.496115
-1031.380205	1.954689	4.506112
-1029.428180	-2.482148	4.516109
-1027.489719	-0.970586	4.526106
-1025.680208	-1.784679	4.536102
-1023.661287	3.639224	4.546099
-1021.680064	-2.130153	4.556096
-1019.953435	-2.976774	4.566093
-1018.453328	-9.709707	4.576090
-1016.449603	-3.058125	4.586086
-1014.342695	1.123310	4.596083
-1012.459468	-0.000979	4.606080
-1010.457084	-0.939065	4.616077
-1008.531970	-3.176876	4.626074
-1006.773933	-6.164795	4.636070
-1004.967557	0.665203	4.646067
-1003.292106	-4.092112	4.656064
-1001.226192	-8.275565	4.666061
-999.229039	-1.016608	4.676058
-997.411813	-3.136105	4.686054
-995.371169	0.588584	4.696051
-993.999275	-6.796453	4.706048
-991.871034	7.148823	4.716045
-989.899635	2.371026	4.726042
-988.056550	0.350030	4.736038
-986.331316	2.318881	4.746035
-984.277986	2.970542	4.756032
-982.321924	-4.032657	4.766029
-980.670837	-3.165087	4.776026
-978.784694	-3.058255	4.786022
-976.798111	6.103444	4.796019
-974.763969	3.091917	4.806016
-972.831685	3.031904	4.816013
-971.154923	4.264844	4.826010
-969.152222	7.507738	4.836006
-967.735745	2.616600	4.846003
-965.670597	9.026311	4.856000
-963.771179	6.459489	4.865997
-961.820122	6.301748	4.875994
-959.720618	3.551356	4.885990
-958.024961	5.733377	4.895987
-956.353173	2.590340	4.905984
-954.488748	3.179080	4.915981
-952.455791	0.066711	4.925978
-950.298255	-4.875027	4.935974
-948.663185	5.018689	4.945971
-946.811204	6.313626	4.955968
-944.884616	3.320902	4.965965
-942.834844	1.838461	4.975962
-941.141696	-4.047416	4.985958
-939.272184	6.277760	4.995955
-937.294682	8.158941	5.005952
-935.655818	5.232759	5.015949
-933.999331	0.069580	5.025946
-931.537043	-5.595074	5.035942
-929.691600	-1.341750	5.045939
-928.218341	-1.194118	5.055936
-926.253548	0.660683	5.065933
-924.246362	-0.585987	5.075930
-922.534163	-1.973380	5.085926
-920.495769	3.340138	5.095923
-918.441601	6.794319	5.105920
-917.071040	5.141035	5.115917
-914.935568	7.668020	5.125914
-913.094400	11.437315	5.135910
-910.962968	-0.581705	5.145907
-909.454803	-0.452273	5.155904
-907.267899	7.430110	5.165901
-905.387539	2.082734	5.175898
-903.710622	5.666721	5.185894
-901.878542	7.569606	5.195891
-899.937174	12.548138	5.205888
-897.705597	9.201952	5.215885
-896.194530	1.510502	5.225882
-894.168734	4.563457	5.235878
-892.418386	0.983172	5.245875
-890.679450	6.175653	5.255872
-888.663660	7.416026	5.265869
-886.872768	2.400332	5.275866
-884.728534	4.648054	5.285862
-883.022322	-1.519345	5.295859
-881.061252	8.267043	5.305856
-879.385442	0.576105	5.315853
-877.298172	4.999229	5.325850
-875.685645	5.273047	5.335846
-873.384769	7.573104	5.345843
-871.533845	-4.964712	5.355840
-869.797578	2.265027	5.365837
-867.906615	4.921147	5.375834
-866.224370	1.187560	5.385830
-864.446048	4.700101	5.395827
-862.763944	4.917016	5.405824
-860.510969	6.814222	5.415821
-858.434027	4.135419	5.425818
-856.551992	3.464596	5.435814
-854.357994	-0.455006	5.445811
-853.014423	4.391769	5.455808
-851.676268	6.463658	5.465805
-849.227670	1.971257	5.475802
-847.090360	5.900101	5.485798
-845.344405	1.406351	5.495795
-843.994276	3.796852	5.505792
-841.732879	10.555830	5.515789
-839.485356	5.389802	5.525786
-838.017748	1.027397	5.535782
-836.103425	3.240867	5.545779
-834.180247	9.198142	5.555776
-832.506268	8.889015	5.565773
-830.485482	2.743992	5.575770
-828.460043	4.268661	5.585766
-826.612871	4.523950	5.595763
-824.893761	13.011722	5.605760
-822.965237	5.013579	5.615757
-820.951182	10.520554	5.625754
-819.143669	8.674319	5.635750
-817.186698	1.724780	5.645747
-815.565817	13.735063	5.655744
-813.706687	4.715400	5.665741
-811.681813	9.950658	5.675738
-810.029290	10.808648	5.685734
-807.970159	8.247996	5.695731
-806.232857	10.346107	5.705728
-804.349062	8.184535	5.715725
-802.268019	6.804583	5.725722
-800.286274	3.067375	5.735718
-798.609250	4.939866	5.745715
-796.514641	10.050307	5.755712
-794.561944	0.322554	5.765709
-792.921551	5.224552	5.775706
-791.166905	4.591512	5.785702
-788.849322	-2.636695	5.795699
-787.578592	3.563854	5.805696
-785.666625	0.720433	5.815693
-783.789063	-1.318548	5.825690
-781.583085	0.535721	5.835686
-779.642757	1.335098	5.845683
-777.821840	-0.358513	5.855680
-776.051377	7.162678	5.865677
-774.048748	5.428973	5.875674
-772.278332	2.091877	5.885670
-770.561782	2.126513	5.895667
-768.599535	1.772935	5.905664
-766.699953	4.672496	5.915661
-764.479915	4.023510	5.925658
-762.830826	0.009506	5.935654
-761.068939	1.271625	5.945651
-759.593706	1.411154	5.955648
-757.257285	-0.457992	5.965645
-755.046905	-0.903322	5.975642
-753.542893	-2.669420	5.985638
-751.843043	-0.191078	5.995635
-749.673203	-2.684110	6.005632
-748.121623	-1.800470	6.015629
-745.995712	-0.031264	6.025626
-743.692584	-3.684001	6.035622
-742.385868	-7.276959	6.045619
-740.470771	-5.267216	6.055616
-738.522192	-2.558619	6.065613
-736.612652	-3.052166	6.075610
-734.807372	-4.586931	6.085606
-733.108835	-3.409403	6.095603
-731.141253	0.042997	6.105600
-729.307534	0.807350	6.115597
-727.085787	-2.663421	6.125594
-725.133793	1.299891	6.135590
-723.265020	-3.194454	6.145587
-722.018920	-2.727760	6.155584
-719.667979	0.147074	6.165581
-718.018308	-6.314333	6.175578
-716.080543	-8.724457	6.185574
-714.085661	-4.629046	6.195571
-712.249763	-4.346602	6.205568
-710.286246	-1.586685	6.215565
-708.443141	-7.243744	6.225562
-706.643761	-0.458164	6.235558
-704.958992	-3.547841	6.245555
-702.693361	0.562735	6.255552
-701.098160	1.087334	6.265549
-698.911509	-2.311488	6.275546
-697.150058	-3.940272	6.285542
-695.374154	-4.178748	6.295539
-693.586346	-5.279642	6.305536
-691.371937	2.088569	6.315533
-689.887200	-8.495891	6.325530
-687.684779	-7.346747	6.335526
-685.896171	-3.376240	6.345523
-684.025839	-6.912392	6.355520
-682.502784	-8.105180	6.365517
-680.583846	-8.099662	6.375514
-678.524125	-4.699836	6.385510
-676.352176	-4.821586	6.395507
-674.989215	-3.227238	6.405504
-672.830577	-5.121575	6.415501
-670.880978	-2.386242	6.425498
-668.954670	-4.710815	6.435494
-667.197332	-9.274151	6.445491
-665.364579	-3.199652	6.455488
-663.580915	-5.953002	6.465485
-661.266002	-5.614430	6.475482
-659.782269	-9.251419	6.485478
-657.773218	-5.696637	6.495475
-656.208429	-7.210283	6.505472
-654.171811	-0.040992	6.515469
-652.028560	-6.246492	6.525466
-650.304376	-9.194009	6.535462
-648.533796	-8.945289	6.545459
-646.598800	-8.006004	6.555456
-644.641826	-8.488109	6.565453
-643.037910	-6.597509	6.575450
-640.885633	-4.156637	6.585446
-638.863086	-2.231871	6.595443
-637.238744	-3.017660	6.605440
-635.296317	-2.057447	6.615437
-633.191445	-2.285281	6.625434
-631.479900	-4.065516	6.635430
-629.934433	-10.099694	6.645427
-628.101543	-8.318300	6.655424
-625.959955	-3.993620	6.665421
-623.845068	-6.916703	6.675418
-622.240226	-8.480936	6.685414
-620.468073	-6.350361	6.695411
-618.368054	-7.426872	6.705408
-616.470670	-6.364711	6.715405
-614.690597	1.033498	6.725402
-612.659871	-11.254980	6.735398
-610.976186	-5.922401	6.745395
-608.824766	-7.485532	6.755392
-607.207777	-8.797488	6.765389
-605.590814	-5.138964	6.775386
-603.393239	-7.911031	6.785382
-601.455579	-7.521602	6.795379
-599.633605	-11.850482	6.805376
-597.886312	-7.096472	6.815373
-596.042030	-4.727929	6.825370
-593.966742	0.428419	6.835366
-591.934714	-5.986628	6.845363
-590.408220	-8.272527	6.855360
-588.527300	-1.233036	6.865357
-586.680829	-6.876335	6.875354
-584.411742	-8.486663	6.885350
-582.681589	-12.971386	6.895347
-580.878656	-14.995129	6.905344
-579.157830	-7.724796	6.915341
-577.421718	-8.880502	6.925338
-575.342874	1.147879	6.935334
-573.212400	-0.847660	6.945331
-571.282368	-5.356414	6.955328
-569.663393	0.842318	6.965325
-568.026832	-1.194312	6.975322
-565.837736	-2.392374	6.985318
-563.940832	-3.095340	6.995315
-562.286956	-0.628459	7.005312
-560.267839	-2.645670	7.015309
-558.244014	4.179970	7.025306
-556.466460	-1.752297	7.035302
-554.946044	0.911171	7.045299
-552.661734	4.044713	7.055296
-550.887262	-6.901748	7.065293
-549.130672	3.156033	7.075290
-547.098655	3.963062	7.085286
-545.068555	0.371491	7.095283
-543.407096	0.296672	7.105280
-541.530471	7.542156	7.115277
-539.663868	5.506692	7.125274
-537.776630	4.107401	7.135270
-536.053317	8.491090	7.145267
-534.100088	0.318689	7.155264
-531.700183	5.336402	7.165261
-530.370021	2.598746	7.175258
-528.353729	5.623547	7.185254
-526.517268	1.753450	7.195251
-524.517042	5.928706	7.205248
-523.138729	7.555430	7.215245
-520.690644	3.614484	7.225242
-518.693019	8.191210	7.235238
-517.313797	6.085193	7.245235
-515.252814	5.439740	7.255232
-513.336873	1.541168	7.265229
-511.411785	-1.465185	7.275226
-509.838451	0.274079	7.285222
-507.741126	-1.322953	7.295219
-505.623800	-2.530023	7.305216
-504.043254	0.644923	7.315213
-502.164317	-2.090370	7.325210
-500.304423	0.777858	7.335206
-498.118788	2.900908	7.345203
-496.556683	7.190376	7.355200
-494.874658	1.424985	7.365197
-492.732536	-1.481810	7.375194
-491.070462	-0.233544	7.385190
-488.802088	-6.777836	7.395187
-486.945913	-4.109529	7.405184
-485.314489	-4.119511	7.415181
-483.235429	-5.629920	7.425178
-481.399404	1.945779	7.435174
-479.696992	-2.534447	7.445171
-477.482903	4.819824	7.455168
-475.930562	-1.460101	7.465165
-474.004119	0.461212	7.475162
-471.888249	-1.375591	7.485158
-470.633808	-6.144261	7.495155
-468.146334	-2.043618	7.505152
-466.360927	-0.818190	7.515149
-464.535681	-3.516458	7.525146
-462.840548	-6.438680	7.535142
-460.706644	-5.894163	7.545139
-458.705633	-2.577917	7.555136
-457.232751	0.296891	7.565133
-455.183310	-2.244546	7.575130
-453.279741	-0.753770	7.585126
-451.467616	-0.457853	7.595123
-449.619632	4.403355	7.605120
-447.562877	-5.356553	7.615117
-445.867022	-5.354693	7.625114
-444.022026	-5.654541	7.635110
-442.115391	-2.427418	7.645107
-440.162604	-1.637644	7.655104
-438.194883	1.096574	7.665101
-436.467964	-2.858594	7.675098
-434.400415	-7.807621	7.685094
-432.504558	-0.298278	7.695091
-430.731320	-9.318164	7.705088
-429.002749	1.544712	7.715085
-427.128370	0.018089	7.725082
-425.203147	-0.008769	7.735078
-423.403248	-3.893477	7.745075
-421.329827	-7.608704	7.755072
-419.467874	-3.630750	7.765069
-417.892870	-2.712735	7.775066
-415.906230	-2.370449	7.785062
-414.094913	-4.959088	7.795059
-411.793428	-4.420761	7.805056
-410.278360	0.362589	7.815053
-408.422573	-3.246824	7.825050
-406.077221	-2.781811	7.835046
-404.446224	-9.175303	7.845043
-402.622422	-4.674931	7.855040
-400.788720	-0.416135	7.865037
-398.957436	-1.042178	7.875034
-396.773810	-0.622383	7.885030
-395.184072	-3.207206	7.895027
-393.168457	-8.204749	7.905024
-391.472180	-7.756079	7.915021
-389.772346	0.831437	7.925018
-387.596916	-2.044269	7.935014
-385.689410	-5.003507	7.945011
-384.171073	-7.161662	7.955008
-382.014904	-1.568035	7.965005
-379.930020	1.666994	7.975002
-377.893228	0.525000	7.984998
-376.608234	-0.072220	7.994995
-374.525999	4.855858	8.004992
-372.718267	-3.689505	8.014989
-370.797120	-2.444625	8.024986
-368.715133	-1.905945	8.034982
-366.865541	-0.131746	8.044979
-364.985486	-0.299763	8.054976
-363.541192	-2.790292	8.064973
-361.565394	-3.156750	8.074970
-359.681695	-3.819552	8.084966
-357.462051	4.389736	8.094963
-355.719885	1.059027	8.104960
-353.765365	1.209127	8.114957
-351.798505	1.114102	8.124954
-350.167068	-2.453133	8.134950
-348.408127	3.309737	8.144947
-346.225354	8.772840	8.154944
-344.692948	-0.497491	8.164941
-342.558819	-1.007632	8.174938
-340.659512	4.554415	8.184934
-338.787634	3.854043	8.194931
-337.077798	-1.656740	8.204928
-335.189666	-3.586538	8.214925
-333.020619	0.920352	8.224922
-331.354346	-3.520848	8.234918
-329.515260	-0.971263	8.244915
-327.698998	-7.987966	8.254912
-325.676514	0.295461	8.264909
-323.766989	-3.109313	8.274906
-322.198036	-1.072381	8.284902
-319.927280	-1.815892	8.294899
-317.866336	-1.292756	8.304896
-316.549050	-3.267195	8.314893
-314.384228	-1.704330	8.324890
-312.451532	0.544537	8.334886
-310.645385	-1.831624	8.344883
-309.139469	-2.246183	8.354880
-307.059028	-0.314580	8.364877
-305.094470	0.471848	8.374874
-303.244478	3.022871	8.384870
-301.423598	7.981688	8.394867
-299.248923	-1.316939	8.404864
-297.390764	-4.876123	8.414861
-296.059867	-1.375391	8.424858
-294.018192	4.364495	8.434854
-291.886941	2.116447	8.444851
-289.769706	-2.169348	8.454848
-288.230119	-1.667170	8.464845
-286.496468	-0.504394	8.474842
-284.280040	-1.474461	8.484838
-282.683712	2.786009	8.494835
-280.818324	-0.314846	8.504832
-278.969335	-1.857829	8.514829
-276.808078	1.147210	8.524826
-274.947906	1.165594	8.534822
-273.035654	-4.009566	8.544819
-271.355753	-2.143467	8.554816
-269.627991	3.371814	8.564813
-267.325475	-2.345635	8.574810
-265.746973	-1.456498	8.584807
-263.833201	-0.134564	8.594803
-261.857778	-2.534553	8.604800
-260.027611	6.430160	8.614797
-258.290334	8.809740	8.624794
-256.597207	1.980103	8.634791
-254.407670	3.229606	8.644787
-252.329617	7.657942	8.654784
-250.810095	2.392327	8.664781
-249.062183	-2.556058	8.674778
-246.528114	-2.391009	8.684775
-245.074006	-4.238829	8.694771
-242.990870	-6.057577	8.704768
-241.346216	0.675720	8.714765
-239.591722	3.140986	8.724762
-237.499944	-0.583338	8.734759
-235.675331	-1.105560	8.744755
-234.041189	-0.413177	8.754752
-231.972740	-3.049040	8.764749
-230.201324	-3.919608	8.774746
-228.124454	-0.796846	8.784743
-226.130098	-1.579837	8.794739
-224.275593	-4.156284	8.804736
-222.654846	-2.604391	8.814733
-220.812576	1.146345	8.824730
-218.475241	-3.193466	8.834727
-216.848964	-6.224531	8.844723
-215.181458	-4.129047	8.854720
-213.081733	-0.874130	8.864717
-211.384608	3.100305	8.874714
-209.318506	-4.031983	8.884711
-207.439661	-1.354437	8.894707
-205.688298	1.637141	8.904704
-203.534237	-10.858623	8.914701
-201.815898	-5.665471	8.924698
-199.844567	-7.807389	8.934695
-198.075488	-8.159669	8.944691
-196.335395	-6.331544	8.954688
-194.497847	-8.373160	8.964685
-192.346268	-8.227536	8.974682
-190.473148	-6.333795	8.984679
-188.768286	-9.947380	8.994675
-186.795184	-5.871710	9.004672
-184.906256	-9.377300	9.014669
-183.170292	-15.770038	9.024666
-181.501502	-11.277907	9.034663
-179.403533	-11.908449	9.044659
-177.360268	-11.933419	9.054656
-175.493081	-9.325040	9.064653
-174.026660	-8.961111	9.074650
-172.219462	-10.009451	9.084647
-169.968443	-10.048623	9.094643
-167.939089	-14.579234	9.104640
-166.420076	-10.205295	9.114637
-164.345713	-4.195776	9.124634
-162.266564	-2.928572	9.134631
-160.455722	-10.479556	9.144627
-158.924319	-2.624447	9.154624
-156.988638	-1.384870	9.164621
-155.193485	-5.947574	9.174618
-153.009590	-4.618130	9.184615
-151.102532	-4.123977	9.194611
-149.274833	-6.253987	9.204608
-147.704734	-5.207116	9.214605
-145.722170	0.226548	9.224602
-143.812096	3.688634	9.234599
-141.834087	-7.241105	9.244595
-139.819910	-7.779294	9.254592
-138.119738	-3.282663	9.264589
-136.138280	-7.014560	9.274586
-134.419431	-8.618771	9.284583
-132.571174	-3.435243	9.294579
-130.455492	-7.583289	9.304576
-128.612197	-4.631586	9.314573
-126.949273	-4.941612	9.324570
-125.025681	0.583585	9.334567
-122.909543	-7.758192	9.344563
-121.222218	-9.276838	9.354560
-119.677328	-5.173835	9.364557
-117.370027	-1.825638	9.374554
-115.514618	0.263621	9.384551
-113.940018	0.024539	9.394547
-111.757250	0.421047	9.404544
-109.953107	-4.525164	9.414541
-108.098270	3.508903	9.424538
-106.170789	2.334051	9.434535
-104.389369	-1.263273	9.444531
-102.390124	4.486715	9.454528
-100.368004	5.133076	9.464525
-98.872776	1.248262	9.474522
-96.931266	3.614323	9.484519
-94.833860	0.981846	9.494515
-92.899958	5.130171	9.504512
-91.283970	4.077661	9.514509
-89.457231	-0.245303	9.524506
-87.337478	0.334966	9.534503
-85.609833	-1.324300	9.544499
-83.598976	6.942265	9.554496
-81.829533	-1.405748	9.564493
-79.842494	-1.232192	9.574490
-78.143839	1.831050	9.584487
-76.297953	3.208177	9.594483
-74.195141	6.413783	9.604480
-72.372601	0.204665	9.614477
-70.543008	3.025971	9.624474
-68.447903	10.671218	9.634471
-66.888052	2.893492	9.644467
-65.232196	-3.963234	9.654464
-63.029948	-2.330321	9.664461
-61.209321	9.353445	9.674458
-59.250026	4.071462	9.684455
-57.905411	1.562274	9.694451
-55.398909	-2.524904	9.704448
-53.352514	-3.117108	9.714445
-51.935866	-0.286751	9.724442
-50.060767	0.439949	9.734439
-47.940426	-0.132469	9.744435
-45.917237	-4.748846	9.754432
-44.343905	-4.253472	9.764429
-42.663459	-1.193616	9.774426
-40.426099	1.938449	9.784423
-38.631403	-3.194100	9.794419
-36.894935	-0.024756	9.804416
-34.968923	-3.532993	9.814413
-33.130993	-6.400338	9.824410
-31.116407	-0.095368	9.834407
-29.274072	8.899182	9.844403
-27.250119	1.101127	9.854400
-25.498202	-1.684597	9.864397
-23.841277	0.472713	9.874394
-21.617602	7.604863	9.884391
-19.796902	-0.858655	9.894387
-18.259323	-2.310712	9.904384
-16.125670	-1.356810	9.914381
-14.258443	4.692210	9.924378
-12.662917	-0.795391	9.934375
-10.676178	3.886151	9.944371
-8.650060	4.315636	9.954368
-6.823251	0.403245	9.964365
-5.010687	13.188873	9.974362
-3.700028	33.440884	9.984359
-2.574242	77.888242	9.994355
-1.111894	125.515753	10.004352
0.000000	177.957452	10.009357
0.935405	215.944844	10.014362
1.326240	248.296448	10.019367
2.070802	259.621381	10.024371
2.150701	280.122982	10.029376
2.894824	293.348241	10.034381
3.023530	307.493275	10.039386
2.979570	317.802316	10.044391
3.223261	321.175748	10.049395
3.662311	319.812374	10.054400
3.645028	316.738251	10.059405
3.393038	322.718615	10.064410
3.299880	324.002692	10.069415
3.883743	339.182178	10.074419
3.740242	358.983086	10.079424
3.855851	352.416863	10.084429
4.001849	351.423509	10.089434
3.786038	359.118582	10.094439
4.262525	345.277042	10.099443
3.755974	340.005405	10.104448
3.952526	339.838199	10.109453
4.074816	344.043136	10.114458
3.798704	348.472474	10.119463
4.090847	362.006438	10.124467
4.181649	380.738667	10.129472
4.346571	375.651646	10.134477
4.477951	371.000489	10.139482
4.462896	380.525944	10.144487
4.566617	362.479737	10.149491
4.088958	353.984904	10.154496
4.213191	371.221559	10.159501
4.400221	375.652723	10.164506
4.479071	386.684974	10.169511
4.697269	385.676947	10.174515
4.431628	391.445048	10.179520
4.486271	394.913309	10.184525
4.737317	398.209891	10.189530
4.687055	398.403757	10.194535
4.977153	390.458223	10.199539
4.860981	399.572463	10.204544
5.241294	401.186303	10.209549
5.125228	392.933393	10.214554
4.596376	404.240790	10.219559
5.142930	388.702255	10.224563
5.099737	405.222906	10.229568
5.141211	407.751820	10.234573
4.985618	401.629386	10.239578
5.137028	399.811988	10.244583
5.222997	408.662175	10.249587
4.934342	418.575077	10.254592
5.266656	413.032407	10.259597
5.236887	412.899725	10.264602
5.002368	418.211860	10.269607
5.296466	404.208545	10.274611
5.274695	411.620378	10.279616
5.380723	410.970867	10.284621
5.458623	414.842281	10.289626
5.286037	418.488720	10.294631
5.453083	429.850715	10.299635
5.282961	444.510331	10.304640
5.911479	439.976974	10.309645
5.740130	446.663624	10.314650
5.691035	450.004940	10.319655
5.979159	447.512863	10.324659
5.605448	449.879351	10.329664
5.595585	446.624242	10.334669
6.007678	451.705512	10.339674
5.734399	455.524142	10.344679
5.961363	446.152027	10.349683
5.880283	457.399080	10.354688
6.024458	451.798095	10.359693
6.437864	458.579134	10.364698
6.064370	472.906939	10.369703
6.546107	475.703111	10.374707
6.338923	476.464488	10.379712
6.359945	471.884519	10.384717
6.502502	474.879875	10.389722
6.427998	487.223477	10.394727
6.913068	486.201259	10.399731
6.474888	478.095877	10.404736
6.414059	475.864464	10.409741
6.620091	488.377786	10.414746
6.391255	492.451114	10.419751
6.760451	490.021793	10.424755
6.815057	488.632994	10.429760
6.951486	487.395149	10.434765
6.924169	494.607634	10.439770
6.951805	502.128329	10.444775
7.139564	498.086313	10.449779
6.715465	505.513485	10.454784
7.079485	494.952512	10.459789
7.265107	499.065390	10.464794
7.253592	508.144079	10.469799
7.168115	500.242625	10.474803
7.322444	503.838516	10.479808
7.197910	504.727061	10.484813
7.229793	500.897570	10.489818
7.064167	508.742414	10.494823
7.452534	496.933320	10.499827
6.923710	514.327932	10.504832
7.207092	503.048098	10.509837
7.583379	509.543342	10.514842
7.284232	509.535631	10.519847
7.513198	509.424757	10.524851
7.372697	518.528758	10.529856
7.538860	527.544425	10.534861
8.133634	532.369499	10.539866
7.780704	531.507758	10.544871
8.081285	532.270147	10.549875
8.063097	539.170532	10.554880
7.766839	536.013127	10.559885
7.671534	528.255154	10.564890
7.717827	545.606952	10.569895
8.000331	538.118299	10.574899
8.236484	539.409792	10.579904
8.131789	528.671243	10.584909
8.169092	535.064449	10.589914
7.952488	546.408883	10.594919
8.259511	534.953362	10.599923
8.028688	540.802703	10.604928
8.384503	546.366078	10.609933
8.253717	539.518947	10.614938
8.077556	544.889629	10.619943
8.124956	543.358469	10.624947
8.141141	558.398498	10.629952
8.456759	569.561859	10.634957
8.725248	571.020088	10.639962
8.802603	570.804084	10.644967
8.980550	577.946021	10.649971
9.012043	582.081930	10.654976
9.094519	571.649392	10.659981
8.740050	559.597608	10.664986
8.771582	569.819092	10.669991
9.101395	572.995916	10.674995
9.402417	578.011368	10.680000
9.123299	567.314806	10.685005
8.997967	553.433445	10.690010
8.713895	560.075048	10.695015
9.069997	565.207869	10.700019
9.144201	586.972400	10.705024
9.260725	579.027643	10.710029
9.660550	579.365765	10.715034
9.331991	588.272721	10.720039
9.668563	579.983774	10.725043
9.259312	585.793783	10.730048
9.532577	578.789140	10.735053
9.050088	578.812250	10.740058
8.881768	591.965707	10.745063
9.404655	587.734589	10.750067
9.372279	592.779572	10.755072
9.233914	588.811629	10.760077
9.371004	591.494062	10.765082
9.373306	605.446656	10.770087
9.985778	614.194062	10.775091
9.937152	621.738023	10.780096
10.018498	621.622309	10.785101
10.228114	620.110999	10.790106
9.747566	627.022097	10.795111
10.241399	617.657768	10.800115
9.982942	629.729627	10.805120
9.807310	631.837461	10.810125
10.293444	630.452357	10.815130
9.868410	629.447565	10.820135
9.893802	626.850706	10.825139
9.951332	629.635725	10.830144
10.113710	634.561346	10.835149
10.043320	625.919384	10.840154
10.041160	625.739718	10.845159
10.727598	644.096573	10.850163
10.414392	654.317910	10.855168
10.717937	659.202098	10.860173
10.889767	648.578629	10.865178
10.756866	646.161561	10.870183
10.577623	630.386872	10.875187
10.357328	633.798117	10.880192
10.662730	649.388211	10.885197
10.722600	653.544846	10.890202
10.356386	662.967224	10.895207
10.841121	657.559425	10.900211
10.732096	668.126682	10.905216
10.783299	664.522730	10.910221
10.973323	660.745244	10.915226
11.093471	666.977056	10.920231
10.966487	660.509317	10.925235
11.354284	672.933880	10.930240
11.205505	662.620168	10.935245
11.177001	656.881064	10.940250
11.372020	665.199913	10.945255
11.665838	657.788243	10.950259
11.323164	663.494620	10.955264
11.365616	667.004316	10.960269
11.454990	662.099562	10.965274
11.513405	666.002536	10.970279
11.457449	661.300741	10.975283
11.333955	667.981436	10.980288
11.557415	686.055793	10.985293
12.195908	684.892394	10.990298
11.838372	678.701125	10.995303
11.713520	664.087855	11.000307
11.766502	670.078063	11.005312
12.182256	680.705129	11.010317
11.875223	672.965081	11.015322
11.914843	669.705183	11.020327
12.237176	659.647495	11.025331
11.875738	666.743046	11.030336
11.904002	668.398880	11.035341
12.335441	681.070386	11.040346
12.046386	690.336966	11.045351
12.590259	688.742369	11.050355
12.017192	680.961170	11.055360
11.957631	695.240695	11.060365
12.523590	693.366599	11.065370
12.533035	696.496779	11.070375
12.324232	691.092358	11.075379
12.453156	698.778354	11.080384
12.891812	689.457474	11.085389
12.756445	684.627986	11.090394
12.551315	699.468490	11.095399
12.785453	692.764934	11.100403
12.862924	694.835558	11.105408
13.118650	682.462406	11.110413
12.979491	676.004486	11.115418
12.536658	670.000296	11.120423
12.548451	670.802449	11.125427
12.404277	687.921441	11.130432
12.474079	696.695534	11.135437
12.820913	688.846448	11.140442
12.805820	698.430467	11.145447
12.882173	694.820919	11.150451
12.735141	695.375586	11.155456
12.890196	720.004657	11.160461
13.178300	727.400341	11.165466
13.263164	734.246533	11.170471
13.560626	727.465049	11.175475
13.570544	728.650716	11.180480
13.544818	735.908800	11.185485
13.704715	732.309571	11.190490
13.401186	726.628501	11.195495
13.594013	732.129635	11.200499
13.641002	731.224591	11.205504
13.416152	724.321411	11.210509
13.513297	728.538356	11.215514
13.278703	736.400632	11.220519
13.484807	737.761594	11.225523
13.290651	731.056948	11.230528
13.609044	736.807722	11.235533
13.838784	737.999329	11.240538
13.513977	732.602357	11.245543
13.704659	738.895492	11.250547
13.890553	757.359142	11.255552
13.891674	762.040861	11.260557
14.131325	758.050423	11.265562
13.962582	765.687737	11.270567
14.226397	753.352660	11.275571
14.348164	758.365228	11.280576
14.355976	761.513029	11.285581
14.741303	749.428241	11.290586
14.455597	756.068616	11.295591
14.489383	753.044604	11.300595
14.407074	756.314016	11.305600
14.500865	742.263477	11.310605
14.655398	750.480020	11.315610
14.409605	754.412618	11.320615
14.560547	743.489626	11.325619
14.579595	756.651192	11.330624
14.606656	753.984656	11.335629
14.904823	753.514224	11.340634
14.327964	755.149892	11.345639
14.569944	752.546850	11.350643
14.696243	753.150964	11.355648
14.886621	748.846679	11.360653
14.955766	752.471990	11.365658
14.707361	759.133225	11.370663
15.199160	767.628730	11.375667
15.353910	777.975791	11.380672
15.059043	781.288574	11.385677
15.264356	775.250344	11.390682
15.421305	777.349305	11.395687
15.648704	772.261644	11.400691
15.478467	767.410880	11.405696
15.634561	754.829624	11.410701
15.680368	752.029206	11.415706
15.195181	754.874008	11.420711
15.507170	750.670177	11.425715
15.395815	754.931426	11.430720
15.147209	758.206863	11.435725
15.617677	764.611504	11.440730
15.567227	773.687109	11.445735
15.826900	783.610570	11.450739
15.782914	787.809042	11.455744
15.681012	786.348981	11.460749
15.785887	789.918138	11.465754
15.669417	787.179869	11.470759
15.969662	784.793040	11.475763
15.768932	788.043499	11.480768
15.647139	789.682280	11.485773
15.758076	786.524525	11.490778
15.935382	784.821226	11.495783
16.296499	784.843819	11.500787
15.812905	786.500884	11.505792
16.160442	792.351116	11.510797
16.602518	812.281595	11.515802
16.423749	812.981683	11.520807
16.663238	798.182425	11.525811
16.442973	792.928033	11.530816
16.521216	784.000485	11.535821
16.138010	783.499960	11.540826
16.282685	806.655542	11.545831
16.622415	798.525246	11.550835
16.182539	810.143627	11.555840
16.318062	805.379703	11.560845
16.740246	806.288297	11.565850
16.604481	819.261718	11.570855
16.990008	808.113595	11.575859
16.837657	811.804214	11.580864
16.773038	809.161753	11.585869
16.884020	809.624805	11.590874
16.879094	808.720152	11.595879
17.461188	795.952634	11.600883
16.858267	812.476294	11.605888
16.930477	806.544440	11.610893
17.312996	803.642995	11.615898
17.214562	806.758866	11.620903
17.348403	793.482509	11.625907
17.069562	806.920303	11.630912
17.449377	825.323146	11.635917
17.738404	826.420145	11.640922
17.231941	814.785067	11.645927
17.643733	814.236583	11.650931
17.385793	821.815612	11.655936
17.618687	823.156539	11.660941
17.867137	819.363385	11.665946
17.532701	822.395473	11.670951
17.533185	821.896826	11.675955
17.710171	836.659173	11.680960
17.647565	829.737948	11.685965
17.910320	841.143350	11.690970
17.768039	839.407439	11.695975
17.954012	831.951380	11.700979
17.711208	842.407633	11.705984
18.014754	841.171489	11.710989
17.722209	843.414700	11.715994
18.009911	842.833968	11.720999
18.047017	843.384501	11.726003
18.082281	844.269656	11.731008
18.010275	834.381985	11.736013
18.355835	835.862644	11.741018
18.133146	849.025005	11.746023
18.166356	834.585054	11.751027
18.165383	853.501274	11.756032
18.485260	861.937522	11.761037
18.897652	865.402451	11.766042
18.590790	859.836982	11.771047
18.403397	845.331279	11.776051
18.769552	854.939749	11.781056
18.683869	862.087607	11.786061
18.781063	868.695344	11.791066
18.544958	866.540715	11.796071
18.762726	862.533238	11.801075
18.814367	865.644108	11.806080
18.957517	862.847066	11.811085
19.447740	861.466023	11.816090
19.536694	857.206270	11.821095
19.302543	842.255425	11.826099
19.226008	838.001573	11.831104
19.025181	834.015139	11.836109
18.897044	825.596743	11.841114
19.049980	827.638002	11.846119
19.084750	823.125118	11.851123
18.753012	840.501297	11.856128
18.618691	859.888244	11.861133
18.950698	862.240005	11.866138
18.602458	872.662632	11.871143
18.982820	874.265483	11.876147
19.268448	891.579521	11.881152
19.491052	890.080305	11.886157
19.752844	894.346734	11.891162
19.855221	901.707475	11.896167
20.019496	889.028599	11.901171
20.205944	895.606342	11.906176
19.924371	872.613917	11.911181
20.398451	856.365749	11.916186
19.910295	858.766324	11.921191
20.065972	855.427947	11.926195
19.818145	853.822414	11.931200
19.888754	866.296162	11.936205
19.983569	849.469804	11.941210
19.714949	862.161667	11.946215
20.117922	855.322292	11.951219
19.960888	862.415296	11.956224
20.235468	881.722857	11.961229
20.218043	887.464177	11.966234
20.330764	898.817860	11.971239
20.548142	895.406551	11.976243
20.334555	892.314730	11.981248
20.459331	886.631513	11.986253
20.737417	884.650343	11.991258
20.378359	894.249930	11.996263
20.369945	891.254699	12.001267
20.484206	891.671497	12.006272
20.535183	888.414470	12.011277
20.867473	894.032200	12.016282
20.684668	886.089286	12.021287
20.825928	887.388063	12.026291
20.677309	892.792328	12.031296
20.619667	885.722044	12.036301
20.827780	884.057976	12.041306
20.635991	887.269183	12.046311
20.729666	870.941321	12.051315
20.570638	872.450427	12.056320
20.626688	868.881922	12.061325
20.679774	871.033735	12.066330
20.678154	868.807010	12.071335
20.583113	852.029857	12.076339
20.637151	861.342749	12.081344
20.767604	858.121940	12.086349
20.560173	857.992359	12.091354
20.497082	860.407139	12.096359
20.620260	853.459423	12.101363
20.508580	868.037602	12.106368
20.604216	869.633826	12.111373
20.791611	874.777899	12.116378
20.664910	878.929664	12.121383
20.570134	864.208888	12.126387
20.367363	880.372318	12.131392
20.712702	887.113956	12.136397
20.959071	890.171692	12.141402
20.377012	878.748901	12.146407
20.344558	871.616257	12.151411
20.586692	882.318477	12.156416
20.678333	893.655017	12.161421
20.968940	896.057543	12.166426
20.690723	888.872623	12.171431
20.585332	870.568967	12.176435
20.407999	870.314732	12.181440
20.880211	891.314465	12.186445
20.860418	882.206943	12.191450
20.573880	872.880189	12.196455
20.594316	866.734210	12.201459
20.515504	875.760783	12.206464
20.631563	883.286497	12.211469
20.779936	868.891224	12.216474
20.503900	871.921892	12.221479
20.744260	861.959146	12.226483
20.363301	866.638761	12.231488
20.466637	863.942691	12.236493
20.806398	881.593450	12.241498
20.655125	884.872313	12.246503
21.024366	875.065627	12.251507
20.840547	869.888975	12.256512
20.814516	870.231952	12.261517
20.520900	861.797350	12.266522
20.409865	871.710613	12.271527
20.760687	861.541006	12.276531
20.635085	867.714329	12.281536
20.683459	874.547484	12.286541
21.015719	865.462670	12.291546
20.967186	867.942941	12.296551
20.733661	870.476375	12.301555
20.983580	868.155909	12.306560
20.982044	871.947072	12.311565
20.805206	863.566385	12.316570
20.810533	863.104812	12.321575
20.764062	868.606320	12.326579
20.569268	854.248451	12.331584
20.612786	856.147889	12.336589
20.559780	833.448664	12.341594
20.420070	847.477761	12.346599
20.711169	867.571178	12.351603
20.580964	872.114600	12.356608
20.911422	874.362526	12.361613
20.527118	866.902791	12.366618
20.582587	871.588492	12.371623
20.634198	857.539838	12.376627
20.671425	873.887340	12.381632
20.505055	876.687618	12.386637
21.030578	861.162977	12.391642
20.459861	862.053323	12.396647
20.400196	850.673391	12.401651
20.635156	864.869833	12.406656
20.580462	863.165682	12.411661
20.874064	870.863352	12.416666
20.498587	870.923009	12.421671
20.797622	855.637934	12.426675
20.702852	855.657547	12.431680
20.606927	848.823632	12.436685
20.469554	847.020702	12.441690
20.274344	854.187603	12.446695
20.666666	859.800475	12.451699
20.735933	874.308796	12.456704
20.975519	871.665112	12.461709
20.787734	857.747687	12.466714
20.513547	855.518706	12.471719
20.741160	851.350384	12.476723
20.504378	852.673186	12.481728
20.602643	849.056950	12.486733
20.794012	843.263777	12.491738
20.473762	844.454806	12.496743
20.378494	846.458384	12.501747
20.426414	865.041956	12.506752
20.631738	870.060160	12.511757
20.810614	874.592132	12.516762
20.497290	878.809935	12.521767
20.740903	867.607130	12.526771
20.744793	876.696209	12.531776
20.429365	869.353225	12.536781
20.697170	874.345694	12.541786
20.725489	875.921116	12.546791
20.920162	863.893453	12.551795
20.634012	857.665487	12.556800
20.746314	851.217844	12.561805
20.914460	846.196380	12.566810
20.519041	860.491790	12.571815
20.555017	850.465454	12.576819
20.631565	847.797316	12.581824
20.707903	850.363326	12.586829
20.965685	845.961526	12.591834
20.657658	855.672802	12.596839
20.724414	850.632814	12.601843
20.677131	859.823090	12.606848
20.851771	853.565783	12.611853
20.945590	849.311565	12.616858
20.650378	860.501618	12.621863
20.772072	849.657331	12.626867
20.859989	851.885591	12.631872
20.917584	853.352257	12.636877
20.978850	864.006040	12.641882
20.447936	846.377439	12.646887
20.786110	838.163788	12.651891
20.531292	831.170715	12.656896
20.544594	824.770414	12.661901
20.659753	837.347422	12.666906
20.316626	849.847724	12.671911
20.709919	847.845028	12.676915
20.848104	856.262944	12.681920
20.867931	846.122487	12.686925
20.484729	833.303895	12.691930
20.245080	834.054697	12.696935
20.730650	845.877166	12.701939
20.681963	849.820929	12.706944
20.492775	856.466456	12.711949
20.666698	850.065757	12.716954
20.771900	862.980280	12.721959
20.862513	848.833946	12.726963
20.574656	837.818441	12.731968
20.667346	831.586832	12.736973
20.414160	833.181918	12.741978
20.460739	841.505623	12.746983
20.910695	839.689440	12.751987
20.620149	847.496042	12.756992
20.225491	839.746224	12.761997
20.603923	846.739617	12.767002
20.338719	857.940652	12.772007
20.584374	857.163191	12.777011
20.586541	867.634006	12.782016
20.834269	864.944868	12.787021
20.789497	858.039709	12.792026
20.510528	867.973448	12.797031
20.554999	864.741119	12.802035
20.449886	859.536147	12.807040
20.826830	860.182292	12.812045
20.866793	865.009242	12.817050
20.724528	864.473436	12.822055
20.815608	858.223147	12.827059
20.757365	858.208548	12.832064
20.639110	840.958851	12.837069
20.586792	830.738446	12.842074
20.378879	838.714797	12.847079
20.817838	841.268699	12.852083
20.494747	855.368057	12.857088
20.552619	860.100682	12.862093
20.944048	856.007158	12.867098
20.406114	852.703718	12.872103
20.527822	850.441554	12.877107
20.190010	854.888770	12.882112
20.850585	865.812829	12.887117
20.805557	859.295656	12.892122
20.698406	868.240009	12.897127
20.874111	857.912249	12.902131
20.569008	859.506157	12.907136
20.477931	849.012789	12.912141
20.815045	853.467473	12.917146
20.504552	849.708270	12.922151
20.820830	851.318186	12.927155
20.591988	852.901506	12.932160
20.686228	852.925665	12.937165
20.730204	843.068376	12.942170
20.442589	847.665285	12.947175
20.681353	837.661807	12.952179
20.804808	842.585824	12.957184
20.503036	839.132750	12.962189
20.516259	836.540949	12.967194
20.497323	839.655185	12.972199
20.870640	838.422106	12.977203
20.762149	844.480722	12.982208
20.755337	837.828148	12.987213
20.788476	835.788279	12.992218
20.612959	843.843047	12.997223
21.007554	834.953321	13.002227
20.637532	841.496792	13.007232
20.244801	844.345786	13.012237
20.381437	841.589213	13.017242
20.316458	848.093494	13.022247
20.715412	848.575272	13.027251
20.432832	841.856291	13.032256
20.656200	861.326542	13.037261
20.973578	862.497873	13.042266
20.297927	849.074606	13.047271
20.613187	848.538365	13.052275
20.822715	854.563607	13.057280
20.884230	848.860532	13.062285
20.765881	840.356984	13.067290
20.382837	843.278553	13.072295
20.809715	834.637576	13.077299
20.625798	835.754818	13.082304
20.572785	845.023272	13.087309
20.525534	839.416401	13.092314
20.337525	846.733542	13.097319
20.692606	838.714321	13.102323
20.685885	839.300232	13.107328
20.679180	844.778041	13.112333
20.533836	843.990404	13.117338
20.401629	841.734047	13.122343
20.693123	856.312564	13.127347
21.006169	861.591138	13.132352
20.791442	847.933496	13.137357
20.796804	842.501166	13.142362
20.828906	840.803674	13.147367
20.509636	840.508999	13.152371
20.908911	840.506582	13.157376
20.721028	845.174318	13.162381
20.714085	842.407529	13.167386
20.790489	851.019807	13.172391
20.638291	842.179444	13.177395
20.709953	839.540473	13.182400
20.530090	849.264419	13.187405
20.822361	850.373518	13.192410
20.455299	857.348627	13.197415
20.503163	848.976263	13.202419
20.380125	851.264981	13.207424
20.576711	851.088305	13.212429
20.793195	847.803310	13.217434
20.799298	848.623728	13.222439
21.050967	833.819336	13.227443
20.609077	853.381495	13.232448
20.927559	849.193948	13.237453
21.071214	841.948069	13.242458
20.714234	854.540474	13.247463
20.593498	844.737843	13.252467
20.703599	844.082933	13.257472
20.535780	840.476024	13.262477
20.745205	842.968763	13.267482
20.671510	841.784907	13.272487
20.580276	825.384083	13.277491
20.809652	827.148212	13.282496
20.582996	819.273833	13.287501
20.993614	811.917575	13.292506
20.655977	821.015362	13.297511
20.362230	817.695060	13.302515
20.753179	815.557119	13.307520
20.654139	810.983577	13.312525
20.764741	803.424433	13.317530
20.466045	816.206212	13.322535
20.925385	806.317389	13.327539
20.490858	815.954195	13.332544
20.469044	808.679530	13.337549
20.731226	808.672171	13.342554
20.502380	813.948850	13.347559
20.485042	809.726566	13.352563
20.067034	817.687529	13.357568
20.343276	834.479428	13.362573
20.675311	838.026557	13.367578
20.578898	841.763457	13.372583
20.772447	837.584801	13.377587
20.819678	842.462626	13.382592
20.732109	842.632484	13.387597
20.757281	851.434291	13.392602
20.625455	853.517821	13.397607
20.828221	832.914657	13.402611
20.441037	826.130364	13.407616
20.543157	822.817883	13.412621
20.664086	832.798204	13.417626
20.601264	845.867250	13.422631
20.724315	832.966332	13.427635
20.457113	842.276833	13.432640
20.486638	843.254370	13.437645
20.787733	837.140910	13.442650
20.588939	841.132269	13.447655
20.626912	844.059226	13.452659
20.802483	852.370248	13.457664
20.699521	835.302629	13.462669
20.521219	825.452420	13.467674
20.394934	840.036055	13.472679
21.002304	835.704657	13.477683
20.844194	830.905556	13.482688
20.319612	825.806929	13.487693
20.507737	829.845383	13.492698
20.485681	843.833632	13.497703
20.530562	847.355600	13.502707
20.443954	846.069720	13.507712
20.604571	847.538877	13.512717
20.807068	844.551016	13.517722
20.493668	850.112441	13.522727
21.031147	844.743474	13.527731
20.586666	839.961661	13.532736
20.571740	851.750422	13.537741
20.796436	852.001365	13.542746
20.590430	844.795487	13.547751
20.819385	837.365687	13.552755
20.331393	829.679649	13.557760
20.262613	844.400778	13.562765
20.697047	843.979575	13.567770
20.322262	852.823099	13.572775
20.478155	844.241111	13.577779
20.579288	851.029569	13.582784
20.632719	847.742196	13.587789
20.631160	844.193926	13.592794
20.476665	848.667096	13.597799
20.652634	848.999930	13.602803
20.717631	856.458078	13.607808
20.835031	845.974039	13.612813
20.931872	843.286894	13.617818
20.638415	848.129172	13.622823
20.866129	848.725000	13.627827
20.857062	846.718671	13.632832
20.571971	837.656648	13.637837
20.897038	835.783112	13.642842
20.561853	825.186766	13.647847
20.935241	820.159384	13.652851
20.456933	822.383334	13.657856
20.226049	823.374020	13.662861
20.707841	829.860468	13.667866
20.451153	847.822373	13.672871
20.717130	845.753249	13.677875
20.932134	857.003849	13.682880
20.863823	846.431155	13.687885
20.549354	830.258329	13.692890
20.454142	824.801045	13.697895
20.503075	820.954556	13.702899
20.402312	826.366933	13.707904
20.549822	839.091753	13.712909
20.822260	837.067333	13.717914
20.676947	844.834998	13.722919
20.850764	838.596754	13.727923
20.577890	829.460244	13.732928
20.345928	822.250632	13.737933
20.710863	842.321197	13.742938
20.526401	854.097577	13.747943
20.864891	850.321594	13.752947
20.414994	851.288866	13.757952
20.714295	856.497087	13.762957
21.087251	841.063037	13.767962
20.559986	838.798729	13.772967
20.537815	827.149473	13.777971
20.438412	824.354857	13.782976
20.606853	825.032680	13.787981
20.715775	827.393209	13.792986
20.363770	836.136892	13.797991
20.729386	842.884737	13.802995
20.648720	848.574625	13.808000
20.801731	843.131359	13.813005
20.611204	832.138183	13.818010
20.781372	843.719211	13.823015
20.656309	834.327301	13.828019
20.563177	833.092926	13.833024
20.719625	839.650197	13.838029
20.420385	840.964036	13.843034
20.356053	837.884691	13.848039
20.957584	839.942712	13.853043
20.637241	840.044039	13.858048
20.664589	840.632400	13.863053
20.910685	831.812096	13.868058
20.425436	828.574378	13.873063
20.917572	825.534014	13.878067
20.833607	837.452052	13.883072
20.644720	842.411695	13.888077
20.762696	831.053908	13.893082
20.397795	842.128902	13.898087
20.707467	834.082232	13.903091
20.423241	843.374948	13.908096
20.298748	844.181502	13.913101
20.571772	835.121925	13.918106
20.369673	842.892338	13.923111
20.688394	835.885054	13.928115
20.757803	832.970465	13.933120
20.781452	831.788429	13.938125
21.011426	836.335894	13.943130
20.832713	840.628414	13.948135
21.110910	831.107525	13.953139
20.783589	833.176502	13.958144
20.462629	841.588794	13.963149
20.895895	830.645937	13.968154
20.685611	840.983457	13.973159
20.806467	835.095874	13.978163
20.991195	846.742394	13.983168
20.710508	839.609934	13.988173
21.016847	832.926337	13.993178
20.436164	824.332534	13.998183
20.713401	818.722800	14.003187
20.734437	819.042498	14.008192
20.234892	819.370840	14.013210
20.509589	821.444034	14.018227
20.441970	838.301317	14.023245
20.896137	835.716573	14.028263
20.799511	836.449035	14.033280
20.806207	833.882183	14.038298
21.038274	836.799010	14.043315
20.539115	827.083379	14.048333
20.665776	832.779190	14.053351
20.954765	835.266949	14.058368
20.658351	846.925821	14.063386
20.879660	842.847696	14.068403
20.664948	838.601597	14.073421
20.751208	836.855740	14.078439
20.727676	842.083165	14.083456
20.699739	842.950959	14.088474
20.652207	845.311503	14.093491
20.378796	846.638440	14.098509
20.647230	838.585713	14.103527
20.693295	843.798891	14.108544
20.617300	840.244805	14.113562
20.875824	854.564758	14.118579
20.863546	866.035182	14.123597
20.952404	864.030936	14.128615
21.178866	869.308156	14.133632
21.184929	868.927862	14.138650
21.306918	868.216052	14.143667
21.280154	883.245342	14.148685
21.031762	866.277498	14.153703
20.888012	862.399165	14.158720
20.992559	868.499631	14.163738
21.202989	872.324389	14.168755
21.398165	874.740604	14.173773
21.249499	875.858888	14.178791
21.182089	874.008551	14.183808
21.133451	874.366853	14.188826
21.300179	875.751001	14.193843
21.304067	876.212607	14.198861
21.370053	872.083745	14.203879
21.620147	868.527974	14.208896
21.574092	873.554514	14.213914
21.522327	866.389678	14.218931
21.319325	870.145102	14.223949
21.420484	872.798105	14.228967
21.217895	879.606651	14.233984
21.343446	880.854225	14.239002
21.144249	872.715622	14.244019
20.825870	885.777995	14.249037
21.014109	874.184640	14.254055
21.013924	879.592395	14.259072
20.939535	882.186886	14.264090
21.397043	896.610419	14.269107
21.381378	904.630257	14.274125
21.840722	910.144048	14.279143
21.585193	907.666199	14.284160
21.667827	924.900731	14.289178
21.952561	900.739420	14.294195
21.918477	908.468046	14.299213
21.981900	905.771013	14.304231
21.695212	885.526405	14.309248
21.495134	882.399506	14.314266
21.566529	882.334402	14.319283
21.596378	901.084256	14.324301
21.501248	905.679768	14.329319
21.923059	911.666727	14.334336
21.654982	908.585275	14.339354
21.884059	893.965231	14.344371
21.687213	914.140218	14.349389
21.773535	906.169983	14.354407
21.744308	905.315553	14.359424
21.778234	912.982998	14.364442
21.982913	898.550882	14.369459
22.006499	907.171638	14.374477
22.066511	909.644024	14.379495
21.893250	906.341386	14.384512
21.997998	913.365189	14.389530
22.237269	902.916680	14.394547
22.077610	905.977800	14.399565
21.973048	901.570970	14.404583
22.219495	903.543291	14.409600
22.034753	905.376754	14.414618
22.039100	905.143022	14.419635
21.914889	902.309179	14.424653
22.183284	904.130138	14.429671
22.166157	895.975065	14.434688
22.016599	910.703079	14.439706
22.454540	902.061718	14.444723
22.433161	906.478728	14.449741
22.242099	906.853456	14.454759
22.501545	906.295895	14.459776
22.260833	912.017302	14.464794
22.597245	902.731475	14.469811
22.362346	904.547770	14.474829
22.207484	907.696212	14.479847
22.323531	902.503874	14.484864
22.253722	896.932203	14.489882
22.565345	895.782737	14.494899
22.062693	903.611268	14.499917
22.230384	899.859425	14.504935
22.438443	897.471225	14.509952
22.088806	895.363887	14.514970
22.492574	896.815620	14.519987
22.198905	904.310375	14.525005
22.422250	897.150405	14.530023
22.450216	908.944773	14.535040
22.338897	924.583760	14.540058
22.858218	923.822728	14.545075
22.627429	930.445462	14.550093
22.589160	931.028623	14.555111
22.784750	931.596505	14.560128
22.811609	926.677929	14.565146
22.781602	914.743405	14.570163
22.455010	909.593353	14.575181
22.723555	913.640084	14.580199
22.410657	924.523012	14.585216
22.703444	933.523982	14.590234
22.958396	929.968995	14.595251
22.985219	937.363884	14.600269
22.888847	935.258614	14.605287
23.306553	924.179169	14.610304
23.040298	910.976740	14.615322
23.014514	899.999511	14.620339
22.850619	895.990678	14.625357
22.605541	893.613409	14.630375
22.971100	896.564011	14.635392
22.546777	899.727119	14.640410
23.149172	906.732889	14.645427
23.362185	916.457568	14.650445
23.104694	914.495975	14.655463
23.372653	899.816242	14.660480
22.952980	905.739221	14.665498
22.826295	898.070376	14.670515
23.247959	895.704734	14.675533
23.142092	901.856079	14.680551
23.162284	897.231154	14.685568
23.267049	899.325173	14.690586
23.120018	896.737213	14.695603
23.088646	901.583671	14.700621
22.986914	912.502121	14.705639
23.577236	914.510829	14.710656
23.262235	917.541673	14.715674
23.158064	903.957899	14.720691
23.212116	911.782580	14.725709
23.633692	926.716808	14.730727
23.540701	918.262369	14.735744
22.900185	908.157103	14.740762
23.411282	919.861835	14.745779
23.431928	924.357090	14.750797
23.431484	928.929641	14.755815
23.576102	923.359937	14.760832
23.387364	922.663080	14.765850
23.543998	924.634000	14.770867
23.499404	928.670908	14.775885
23.337916	930.823129	14.780903
23.535867	922.910584	14.785920
23.385563	926.506609	14.790938
23.330338	920.904288	14.795955
23.806449	930.450160	14.800973
23.496265	934.763810	14.805991
23.760787	932.649739	14.811008
23.489090	932.593742	14.816026
23.337662	925.633533	14.821043
23.542938	929.916872	14.826061
23.747127	930.942699	14.831079
23.678628	918.481064	14.836096
23.623907	930.505713	14.841114
23.378166	930.355915	14.846131
23.580080	934.830125	14.851149
23.485809	962.641476	14.856167
23.915834	953.743375	14.861184
24.213616	957.632873	14.866202
24.373562	942.326967	14.871219
23.965130	938.569481	14.876237
23.749567	922.118571	14.881255
24.053037	922.293298	14.886272
23.789915	933.766035	14.891290
23.878300	941.063018	14.896307
24.199748	954.457546	14.901325
24.311409	957.140350	14.906343
23.956316	949.805207	14.911360
24.097658	941.843479	14.916378
24.133945	944.709760	14.921395
24.422493	941.748727	14.926413
24.083218	943.548641	14.931431
24.147127	924.179275	14.936448
24.063949	936.409812	14.941466
24.203486	944.669181	14.946483
24.451104	937.519477	14.951501
24.482571	935.428422	14.956519
24.337504	920.053215	14.961536
23.937949	916.332071	14.966554
24.615249	937.361797	14.971571
24.321118	923.481120	14.976589
24.116852	930.370179	14.981607
24.400426	942.303127	14.986624
24.525059	942.495369	14.991642
24.718225	949.190486	14.996659
24.261702	936.153660	15.001677
24.238983	932.792398	15.006695
24.578371	939.849573	15.011712
24.374483	953.522946	15.016730
24.549577	947.141421	15.021747
24.838243	945.229561	15.026765
24.270355	957.482373	15.031783
24.816698	945.216798	15.036800
24.601084	954.588305	15.041818
24.563803	952.448439	15.046835
24.369606	947.760168	15.051853
24.380559	954.680977	15.056871
24.735114	951.018864	15.061888
24.283462	950.217652	15.066906
24.359431	948.128935	15.071923
24.862346	945.267414	15.076941
24.367302	948.908993	15.081959
24.986719	942.398397	15.086976
24.830830	952.002619	15.091994
24.885346	950.543380	15.097011
25.203555	941.877049	15.102029
25.038741	949.064988	15.107047
25.137915	951.051368	15.112064
24.908815	952.655961	15.117082
25.036599	949.300576	15.122099
25.161953	941.044101	15.127117
24.841931	957.808077	15.132135
24.859487	954.725099	15.137152
25.096556	947.621117	15.142170
24.713360	955.889938	15.147187
24.783178	947.184574	15.152205
24.883913	962.744162	15.157223
24.962501	960.365592	15.162240
25.224309	967.273136	15.167258
25.600571	961.375463	15.172275
25.681941	967.043946	15.177293
25.123398	960.227307	15.182311
25.252088	949.370118	15.187328
25.307632	953.708807	15.192346
24.969880	960.554679	15.197363
25.299586	963.893255	15.202381
25.162182	970.008761	15.207399
25.259772	965.813483	15.212416
25.229107	967.136319	15.217434
25.787335	973.650525	15.222451
25.285496	967.965267	15.227469
25.121518	972.659870	15.232487
25.673760	964.948764	15.237504
25.804942	963.802907	15.242522
25.396997	961.752048	15.247539
25.783641	958.515819	15.252557
25.566538	962.783169	15.257575
25.418285	958.364415	15.262592
25.564510	960.171835	15.267610
25.285911	959.533353	15.272627
25.412573	961.557822	15.277645
25.681832	963.306293	15.282663
25.556348	967.299485	15.287680
25.300025	962.334831	15.292698
25.358175	970.081812	15.297715
25.633033	973.155435	15.302733
25.983841	996.019540	15.307751
25.939942	986.740839	15.312768
25.796535	990.917793	15.317786
25.955447	993.119591	15.322803
26.143227	989.589461	15.327821
25.721490	985.138816	15.332839
25.866886	978.395503	15.337856
26.071683	978.505746	15.342874
25.854923	983.479328	15.347891
26.267977	981.915707	15.352909
26.104481	992.008801	15.357927
26.148875	985.044071	15.362944
25.851655	974.610297	15.367962
25.913108	978.579968	15.372979
26.307574	981.884623	15.377997
26.091342	990.962100	15.383015
26.385282	984.742498	15.388032
26.550105	985.346749	15.393050
26.431626	982.401866	15.398067
26.164840	967.541520	15.403085
25.739028	965.586318	15.408103
26.113991	972.694464	15.413120
26.460253	990.187469	15.418138
26.333519	987.490864	15.423155
26.910071	969.927279	15.428173
26.455567	957.497292	15.433191
26.465740	950.888816	15.438208
26.773307	948.544511	15.443226
26.352777	953.295758	15.448243
26.467918	947.030759	15.453261
26.525362	953.396747	15.458279
26.060709	951.439877	15.463296
26.197899	950.999341	15.468314
26.396427	971.644594	15.473331
26.694688	982.175256	15.478349
26.519704	985.152321	15.483367
26.515082	983.795318	15.488384
26.697770	978.173904	15.493402
26.309811	989.973332	15.498419
26.888347	987.795011	15.503437
26.737237	995.057863	15.508455
26.571695	988.633125	15.513472
26.773771	986.739790	15.518490
26.651274	996.013103	15.523507
27.043643	979.204041	15.528525
26.704529	996.688398	15.533543
26.716283	991.363227	15.538560
26.938352	994.731562	15.543578
26.779874	997.219937	15.548595
26.700268	986.870993	15.553613
26.873227	991.087147	15.558631
26.644497	990.900028	15.563648
26.965580	987.694699	15.568666
26.651081	998.533893	15.573683
27.082305	996.416819	15.578701
27.010123	1011.601350	15.583719
26.996823	1017.262930	15.588736
27.455330	1019.173130	15.593754
27.159511	1023.777094	15.598771
27.275608	1018.517067	15.603789
27.166859	1025.350037	15.608807
26.822296	1014.308738	15.613824
26.823578	1018.719022	15.618842
26.936124	1013.933040	15.623859
27.121745	1011.224361	15.628877
26.946114	1018.859221	15.633895
27.158893	1010.557302	15.638912
27.073532	1018.737755	15.643930
27.290643	1034.522674	15.648947
27.856877	1035.051891	15.653965
27.636627	1029.370458	15.658983
27.930198	1021.263285	15.664000
27.853681	1014.816470	15.669018
27.584103	1012.762410	15.674035
27.585687	1008.134126	15.679053
27.603205	1016.144014	15.684071
27.771895	1012.116706	15.689088
27.631226	1003.558138	15.694106
27.268322	1011.721508	15.699123
27.709229	1003.518486	15.704141
27.669665	1009.741097	15.709159
27.712268	1006.717034	15.714176
27.889339	994.895704	15.719194
27.789182	1015.683041	15.724211
28.083955	1008.208033	15.729229
28.088312	1001.830121	15.734247
27.956376	1008.238924	15.739264
28.062175	1011.224691	15.744282
27.850837	1011.656137	15.749299
27.949963	1010.041913	15.754317
27.843343	1009.970595	15.759335
27.848830	1003.106443	15.764352
28.008316	1010.573017	15.769370
27.530956	1011.921487	15.774387
27.701935	1006.879224	15.779405
27.412853	1012.307940	15.784423
27.548563	1031.277030	15.789440
27.972436	1032.947366	15.794458
27.866759	1040.029962	15.799475
27.934850	1040.072349	15.804493
27.911107	1041.939923	15.809511
27.867568	1046.829269	15.814528
28.099702	1042.307345	15.819546
28.144767	1051.491045	15.824563
28.028206	1039.508877	15.829581
28.503783	1048.666380	15.834599
28.225264	1063.835112	15.839616
28.707430	1061.783836	15.844634
28.601475	1054.574068	15.849651
28.283265	1041.604747	15.854669
28.332394	1048.310300	15.859687
28.389195	1054.424753	15.864704
28.747188	1056.605819	15.869722
28.256522	1062.173671	15.874739
28.311622	1068.412669	15.879757
28.592441	1068.595730	15.884775
28.721604	1068.062091	15.889792
29.076831	1062.174025	15.894810
28.859030	1057.682963	15.899827
28.926498	1045.183802	15.904845
28.601051	1030.917908	15.909863
28.746865	1032.127658	15.914880
28.944386	1029.783590	15.919898
28.633119	1036.944594	15.924915
28.903609	1024.579808	15.929933
28.814253	1029.001406	15.934951
28.602872	1027.043453	15.939968
28.827852	1040.720861	15.944986
29.028765	1057.758936	15.950003
29.149781	1048.726022	15.955021
28.884872	1050.627344	15.960039
29.030151	1035.484127	15.965056
28.844220	1024.390776	15.970074
28.705543	1041.012666	15.975091
29.171415	1048.938474	15.980109
29.307042	1055.776525	15.985127
29.064107	1056.261776	15.990144
29.476529	1064.254319	15.995162
29.103095	1042.999293	16.000179
29.174289	1030.985610	16.005197
29.034309	1040.999483	16.010215
29.192147	1050.964287	16.015232
29.276582	1049.541163	16.020250
29.176888	1061.042988	16.025267
29.086267	1056.347599	16.030285
29.245064	1047.695621	16.035303
29.374407	1056.697570	16.040320
29.671282	1050.947804	16.045338
29.172720	1057.438700	16.050355
29.540142	1062.501601	16.055373
29.169731	1067.317249	16.060391
28.877173	1062.070478	16.065408
29.547026	1063.773942	16.070426
29.111741	1060.217334	16.075443
29.366775	1056.558485	16.080461
29.645444	1061.228130	16.085479
29.753457	1073.123122	16.090496
29.860294	1059.826441	16.095514
29.529115	1060.371384	16.100531
29.600862	1061.007788	16.105549
29.506208	1082.038159	16.110567
29.675339	1079.799285	16.115584
29.964189	1073.948543	16.120602
29.668302	1084.776967	16.125619
30.018554	1085.205357	16.130637
30.038552	1074.746082	16.135655
29.979116	1081.649864	16.140672
30.112577	1077.057152	16.145690
30.149947	1081.963492	16.150707
30.148752	1074.188021	16.155725
30.116474	1064.465399	16.160743
29.246144	1071.471773	16.165760
30.252977	1076.330446	16.170778
29.924159	1079.426448	16.175795
30.140818	1081.192761	16.180813
30.009236	1073.576513	16.185831
30.070038	1083.438840	16.190848
30.067109	1077.065204	16.195866
29.835965	1085.430968	16.200883
30.299668	1078.259314	16.205901
30.335405	1084.413318	16.210919
30.223815	1082.060344	16.215936
30.426687	1075.290515	16.220954
30.318847	1073.386827	16.225971
30.358971	1087.606568	16.230989
30.753529	1077.307771	16.236007
30.468562	1085.074935	16.241024
30.620835	1071.597964	16.246042
30.860436	1079.065952	16.251059
30.839184	1075.932510	16.256077
30.757268	1085.018509	16.261095
30.122079	1087.626979	16.266112
30.286667	1080.012252	16.271130
30.479649	1084.549281	16.276147
30.433310	1088.775274	16.281165
30.639335	1087.037026	16.286183
30.659535	1088.532656	16.291200
30.575197	1077.992493	16.296218
30.699028	1080.635627	16.301235
30.733901	1088.098522	16.306253
31.020916	1088.710030	16.311271
30.920449	1094.025322	16.316288
30.689580	1084.807840	16.321306
30.783093	1094.152153	16.326323
31.062435	1103.938739	16.331341
31.464723	1096.643165	16.336359
31.005393	1093.950825	16.341376
31.185022	1079.486346	16.346394
30.724944	1079.155229	16.351411
30.866881	1075.207676	16.356429
31.443565	1086.902085	16.361447
31.083905	1107.298363	16.366464
31.201308	1097.613192	16.371482
31.284997	1100.998905	16.376499
31.209866	1108.388121	16.381517
31.482593	1101.223322	16.386535
31.604898	1085.336532	16.391552
30.962336	1074.588108	16.396570
30.962864	1083.819831	16.401587
30.980592	1098.868990	16.406605
31.212888	1106.372764	16.411623
30.906196	1107.819863	16.416640
31.441383	1106.370456	16.421658
31.247456	1101.257376	16.426675
31.535475	1106.479248	16.431693
31.365627	1097.986625	16.436711
31.256662	1100.237459	16.441728
31.377480	1112.352237	16.446746
31.599294	1124.702599	16.451763
31.961279	1129.431337	16.456781
31.865032	1117.316876	16.461799
31.906190	1114.031899	16.466816
31.877073	1104.423576	16.471834
31.935589	1096.907555	16.476851
31.880712	1091.998814	16.481869
31.962551	1092.059458	16.486887
32.130295	1101.734855	16.491904
32.178980	1094.402874	16.496922
31.957517	1089.320931	16.501939
31.786775	1098.120659	16.506957
32.128931	1094.885205	16.511975
31.870171	1103.400101	16.516992
32.080113	1096.957897	16.522010
32.283180	1089.897022	16.527027
32.207425	1097.004761	16.532045
32.206712	1093.402425	16.537063
31.549956	1089.443834	16.542080
31.933529	1092.116327	16.547098
31.975020	1093.231037	16.552115
31.774146	1094.963276	16.557133
32.300158	1101.290772	16.562151
32.096816	1121.474948	16.567168
32.433944	1118.502985	16.572186
32.495745	1119.498054	16.577203
32.180739	1124.954542	16.582221
32.560570	1122.263630	16.587239
32.496562	1136.094188	16.592256
32.880711	1119.506499	16.597274
32.765678	1122.367064	16.602291
32.151167	1107.118443	16.607309
32.724752	1107.577279	16.612327
32.542934	1120.896505	16.617344
32.763501	1117.974594	16.622362
32.589987	1113.806785	16.627379
32.650229	1122.069466	16.632397
32.503990	1121.941546	16.637415
32.533018	1119.869730	16.642432
32.645978	1115.690834	16.647450
32.763424	1118.202860	16.652467
32.618048	1121.672304	16.657485
33.170733	1114.566665	16.662503
32.819786	1115.624421	16.667520
32.446777	1121.909703	16.672538
32.948442	1120.991032	16.677555
32.691690	1122.784096	16.682573
32.826236	1111.647428	16.687591
32.620856	1121.431114	16.692608
32.534038	1122.003150	16.697626
32.911050	1140.751425	16.702643
32.857214	1148.978833	16.707661
33.327753	1148.631415	16.712679
33.124731	1143.806060	16.717696
33.189835	1152.058544	16.722714
33.333435	1141.917706	16.727731
33.298438	1151.026150	16.732749
33.681058	1146.568282	16.737767
33.391777	1149.826305	16.742784
33.360040	1146.637891	16.747802
33.495760	1145.985226	16.752819
33.171899	1150.142243	16.757837
33.664863	1150.149898	16.762855
33.565320	1145.479497	16.767872
33.559313	1148.673462	16.772890
33.835122	1144.204316	16.777907
33.365267	1146.410472	16.782925
33.522001	1140.892235	16.787943
33.392005	1144.352940	16.792960
33.544445	1135.533611	16.797978
33.502277	1142.019390	16.802995
33.305415	1149.929838	16.808013
33.662875	1139.452871	16.813031
33.898160	1141.208356	16.818048
33.805970	1138.883738	16.823066
34.054278	1141.752421	16.828083
33.544452	1133.405239	16.833101
33.946914	1145.476696	16.838119
33.738182	1146.848398	16.843136
33.720965	1141.279255	16.848154
33.855795	1154.236548	16.853171
33.653394	1171.765376	16.858189
34.209458	1165.676922	16.863207
34.381207	1168.063890	16.868224
34.203585	1170.116473	16.873242
34.053705	1168.147118	16.878259
34.242475	1171.719008	16.883277
34.293284	1168.525288	16.888295
34.101488	1174.888655	16.893312
34.194963	1165.904107	16.898330
34.520352	1163.561645	16.903347
34.449870	1173.710815	16.908365
34.543200	1169.851214	16.913383
34.562554	1173.854395	16.918400
34.545146	1174.704799	16.923418
34.635685	1170.169241	16.928435
34.257469	1176.979195	16.933453
34.108181	1158.172059	16.938471
34.469263	1165.507459	16.943488
34.143040	1168.334077	16.948506
34.439017	1165.187770	16.953523
34.150192	1175.109071	16.958541
34.413635	1168.534033	16.963559
34.591943	1184.279688	16.968576
34.699360	1192.180952	16.973594
35.104531	1189.117898	16.978611
34.703702	1198.308317	16.983629
35.203087	1186.145986	16.988647
35.054662	1195.456594	16.993664
34.790829	1177.318938	16.998682
35.412035	1177.985687	17.003699
34.882010	1167.128007	17.008717
34.800563	1160.787307	17.013735
35.115169	1179.688732	17.018752
35.081039	1189.935935	17.023770
35.163841	1183.635094	17.028787
35.145735	1189.220429	17.033805
35.490753	1182.890350	17.038823
35.314951	1178.504236	17.043840
35.224460	1163.794893	17.048858
35.501183	1151.815970	17.053875
35.091348	1163.615881	17.058893
35.127016	1163.745238	17.063911
35.408675	1166.356922	17.068928
35.447605	1184.841427	17.073946
35.306622	1187.781649	17.078963
35.176282	1192.986910	17.083981
35.420615	1189.620746	17.088999
35.312628	1195.289632	17.094016
35.295704	1194.179964	17.099034
35.661679	1186.750139	17.104051
35.158266	1191.972432	17.109069
35.581231	1190.152380	17.114087
35.575299	1185.876024	17.119104
35.493198	1182.977207	17.124122
35.652565	1184.508852	17.129139
35.499031	1191.750166	17.134157
35.760655	1203.875596	17.139175
36.009167	1207.667630	17.144192
36.190601	1213.774855	17.149210
36.236859	1197.860746	17.154227
35.974855	1201.469935	17.159245
35.748589	1188.940421	17.164263
35.542875	1189.413446	17.169280
36.121839	1205.044883	17.174298
36.445728	1204.981977	17.179315
36.030797	1202.427253	17.184333
36.277110	1212.003675	17.189351
36.538279	1215.011895	17.194368
36.054024	1198.557907	17.199386
36.392026	1194.277028	17.204403
36.004625	1191.699038	17.209421
36.256892	1208.194270	17.214439
36.568834	1204.162938	17.219456
36.236864	1213.236990	17.224474
36.204324	1211.264644	17.229491
36.135361	1210.529792	17.234509
36.271592	1206.655473	17.239527
36.532092	1214.354580	17.244544
36.412615	1219.039018	17.249562
36.495765	1208.534967	17.254579
36.399328	1211.416178	17.259597
36.194464	1216.730862	17.264615
36.213141	1211.951922	17.269632
36.508306	1225.983255	17.274650
36.796343	1236.102027	17.279667
36.633298	1238.134991	17.284685
36.935197	1234.608623	17.289703
37.172264	1239.804065	17.294720
36.755103	1249.207907	17.299738
37.063441	1234.699150	17.304755
37.320692	1237.514516	17.309773
37.101363	1237.769489	17.314791
37.408510	1226.292169	17.319808
37.361202	1225.851165	17.324826
37.228894	1210.739455	17.329843
37.232158	1209.695780	17.334861
37.050009	1208.791789	17.339879
37.110332	1202.220818	17.344896
36.906901	1210.267627	17.349914
37.196931	1216.142028	17.354931
37.346496	1227.624677	17.359949
37.362885	1228.763851	17.364967
37.667957	1230.242375	17.369984
37.427844	1222.748751	17.375002
37.440483	1198.918208	17.380019
37.413341	1205.933303	17.385037
37.530470	1223.645611	17.390055
37.752187	1210.410694	17.395072
37.306093	1209.699813	17.400090
37.603387	1216.831481	17.405107
37.790283	1231.833347	17.410125
37.565809	1232.524871	17.415143
37.661893	1226.947062	17.420160
37.543720	1229.653991	17.425178
37.593523	1226.760868	17.430195
37.291035	1230.396970	17.435213
37.480593	1234.009650	17.440231
37.784737	1223.405845	17.445248
37.640143	1230.585978	17.450266
37.906204	1229.863756	17.455283
37.942388	1231.666740	17.460301
37.670276	1229.740467	17.465319
38.197008	1247.277361	17.470336
37.823662	1262.632886	17.475354
38.136059	1260.371134	17.480371
37.827829	1262.896022	17.485389
37.930061	1270.074559	17.490407
38.253984	1266.289839	17.495424
38.009765	1267.467436	17.500442
38.063632	1264.548489	17.505459
38.062925	1259.711276	17.510477
37.830131	1263.199416	17.515495
38.119061	1280.552481	17.520512
38.209933	1290.229253	17.525530
38.246897	1284.719054	17.530547
37.984688	1289.858865	17.535565
38.215017	1295.458100	17.540583
38.651591	1285.295603	17.545600
38.442465	1297.062035	17.550618
38.965425	1285.987553	17.555635
38.675531	1295.059664	17.560653
38.657459	1294.462983	17.565671
38.776660	1291.871814	17.570688
38.487112	1295.516880	17.575706
38.826231	1307.947791	17.580723
38.655334	1319.420277	17.585741
38.826947	1323.248202	17.590759
39.064063	1316.114147	17.595776
39.013164	1326.018051	17.600794
39.282798	1316.209353	17.605811
39.172070	1310.085618	17.610829
39.432422	1308.209690	17.615847
39.246361	1300.968529	17.620864
39.470117	1289.554798	17.625882
39.716753	1281.484855	17.630899
39.437092	1277.503817	17.635917
39.357375	1274.667523	17.640935
39.795548	1281.707539	17.645952
39.472265	1278.831440	17.650970
39.415080	1276.188182	17.655987
39.654490	1271.710646	17.661005
39.629543	1282.757127	17.666023
39.450379	1274.873079	17.671040
39.193806	1275.148150	17.676058
39.523904	1271.821771	17.681075
39.266265	1282.293454	17.686093
39.106414	1275.803185	17.691111
39.524405	1268.053560	17.696128
39.423537	1271.514368	17.701146
39.628334	1288.825805	17.706163
39.878376	1302.571825	17.711181
39.851196	1303.513458	17.716199
39.900445	1301.461987	17.721216
39.843724	1307.923419	17.726234
39.863568	1303.830109	17.731251
39.855341	1312.840002	17.736269
39.863093	1308.674686	17.741287
40.199875	1300.127880	17.746304
39.904183	1313.076903	17.751322
40.017542	1308.303279	17.756339
40.110409	1306.376985	17.761357
40.030036	1311.890501	17.766375
40.220933	1309.800705	17.771392
40.099121	1311.886878	17.776410
40.286480	1301.671309	17.781427
40.203745	1304.632151	17.786445
40.086483	1307.181645	17.791463
40.223007	1302.869949	17.796480
40.239420	1313.784013	17.801498
40.296515	1328.045328	17.806515
40.454588	1332.773624	17.811533
40.387551	1330.342715	17.816551
40.288050	1328.052267	17.821568
40.498242	1334.740130	17.826586
40.561705	1330.771991	17.831603
40.695329	1333.306642	17.836621
40.562280	1334.024487	17.841639
40.676916	1318.734850	17.846656
40.193936	1333.429954	17.851674
40.472669	1341.719259	17.856691
40.727470	1350.710820	17.861709
40.729788	1352.327309	17.866727
41.311062	1364.494701	17.871744
40.860565	1365.529024	17.876762
41.189235	1353.337154	17.881779
41.239730	1350.623224	17.886797
41.326384	1356.885629	17.891815
41.239493	1351.429766	17.896832
41.235190	1360.624683	17.901850
41.339908	1354.230609	17.906867
41.191619	1354.741671	17.911885
41.229325	1355.465316	17.916903
41.642531	1348.844288	17.921920
41.419420	1352.365512	17.926938
41.502567	1355.358110	17.931955
41.531445	1351.065141	17.936973
41.490737	1352.883550	17.941991
41.678072	1340.253330	17.947008
41.567756	1344.538365	17.952026
41.454317	1347.425461	17.957043
41.783481	1346.748227	17.962061
41.608636	1351.935474	17.967079
41.554179	1351.287964	17.972096
41.621983	1353.004121	17.977114
41.583823	1350.961865	17.982131
41.955941	1348.965858	17.987149
41.687801	1347.139611	17.992167
41.907547	1349.165019	17.997184
41.699227	1349.893297	18.002202
41.615887	1351.317379	18.007219
42.058246	1363.063327	18.012237
42.115476	1377.121746	18.017255
42.528017	1375.191648	18.022272
42.630810	1377.847631	18.027290
42.412802	1352.788890	18.032307
42.183750	1342.010490	18.037325
42.003874	1351.140594	18.042343
42.038890	1348.583292	18.047360
42.085589	1366.336895	18.052378
42.037316	1378.390775	18.057395
42.374349	1365.793287	18.062413
42.097710	1368.259670	18.067431
42.324971	1372.388624	18.072448
42.302866	1376.675330	18.077466
42.041099	1377.453033	18.082483
42.574912	1390.420835	18.087501
42.335879	1402.122907	18.092519
42.789832	1397.532462	18.097536
42.679632	1400.414333	18.102554
42.652361	1397.813472	18.107571
43.171090	1394.401924	18.112589
43.002174	1395.507745	18.117607
43.137819	1393.757091	18.122624
42.835976	1402.527575	18.127642
42.808709	1396.242625	18.132659
43.429277	1390.579527	18.137677
43.016163	1397.498970	18.142695
43.122663	1395.765549	18.147712
43.231692	1391.426751	18.152730
43.405917	1390.080511	18.157747
43.271635	1396.341991	18.162765
43.279139	1396.232019	18.167783
43.453257	1396.274801	18.172800
43.401165	1398.173684	18.177818
43.347321	1400.274197	18.182835
43.462812	1392.275447	18.187853
43.410899	1391.451348	18.192871
43.509923	1387.557747	18.197888
43.602934	1389.095280	18.202906
43.372314	1394.178178	18.207923
43.418246	1391.022941	18.212941
43.248600	1395.685548	18.217959
43.579807	1387.016883	18.222976
43.421696	1397.501088	18.227994
43.290308	1405.508199	18.233011
43.964865	1417.371316	18.238029
43.657032	1419.273238	18.243047
43.786696	1414.323942	18.248064
44.264811	1417.275580	18.253082
43.987954	1418.840647	18.258099
44.212403	1414.972653	18.263117
43.844529	1424.461556	18.268135
44.229322	1415.534212	18.273152
44.133765	1417.073508	18.278170
44.173004	1414.249674	18.283187
44.403891	1417.794459	18.288205
44.409932	1421.126564	18.293223
44.579387	1417.201273	18.298240
44.497876	1413.399382	18.303258
44.406775	1422.900770	18.308275
44.406898	1415.581092	18.313293
44.349528	1420.571871	18.318311
44.489170	1421.351623	18.323328
44.363853	1412.801374	18.328346
44.359591	1412.125406	18.333363
44.878159	1407.741733	18.338381
44.681767	1411.235113	18.343399
44.689538	1411.946233	18.348416
44.493156	1426.462009	18.353434
44.652401	1436.779219	18.358451
45.150959	1434.512919	18.363469
44.881533	1441.982058	18.368487
45.202914	1444.527682	18.373504
44.986148	1443.330317	18.378522
44.725721	1449.426318	18.383539
45.116835	1438.283086	18.388557
45.204174	1450.869112	18.393575
45.152178	1446.489912	18.398592
44.701938	1439.758015	18.403610
44.588425	1434.167937	18.408627
44.959282	1443.907125	18.413645
44.703977	1458.183787	18.418663
44.958795	1468.389820	18.423680
45.464476	1471.272578	18.428698
45.387593	1471.493823	18.433715
45.368376	1465.273627	18.438733
45.514695	1470.653517	18.443751
45.553670	1464.551458	18.448768
45.392033	1475.468873	18.453786
45.207687	1470.519304	18.458803
45.762906	1473.147190	18.463821
45.856013	1500.294169	18.468839
45.894052	1499.288972	18.473856
45.841233	1494.930338	18.478874
45.650772	1505.375735	18.483891
46.145338	1495.675763	18.488909
46.027086	1504.621524	18.493927
46.106541	1502.178233	18.498944
46.126357	1501.806741	18.503962
45.901685	1500.322761	18.508979
46.151346	1492.593574	18.513997
45.885778	1502.797685	18.519015
46.267151	1499.061947	18.524032
46.430030	1496.518832	18.529050
46.323228	1499.153210	18.534067
46.505357	1499.326852	18.539085
46.345072	1497.157758	18.544103
46.357062	1496.381664	18.549120
46.332085	1487.853121	18.554138
46.264934	1492.946161	18.559155
46.695063	1490.140195	18.564173
46.292891	1504.989326	18.569191
46.392870	1493.519670	18.574208
46.518790	1504.057754	18.579226
46.507209	1521.828708	18.584243
46.744041	1526.182700	18.589261
46.813940	1527.181226	18.594279
46.667973	1527.842937	18.599296
46.880180	1524.137320	18.604314
47.112858	1532.333405	18.609331
46.876004	1518.649090	18.614349
46.612552	1523.191415	18.619367
47.040186	1527.845321	18.624384
47.204972	1522.415321	18.629402
46.797707	1532.715986	18.634419
47.281478	1545.509434	18.639437
47.565999	1559.769311	18.644455
47.552992	1550.269812	18.649472
47.528213	1540.213757	18.654490
47.234476	1551.400842	18.659507
47.574909	1550.839782	18.664525
47.430762	1556.100859	18.669543
47.757134	1552.320395	18.674560
47.761858	1553.971130	18.679578
47.505417	1558.924493	18.684595
47.704380	1547.083494	18.689613
47.631019	1541.966757	18.694631
47.434348	1545.875503	18.699648
47.512327	1555.479002	18.704666
47.846339	1552.386325	18.709683
47.559169	1543.813048	18.714701
47.459426	1554.143334	18.719719
47.532866	1549.777131	18.724736
48.211339	1565.551970	18.729754
47.975945	1583.987138	18.734771
48.101963	1580.890661	18.739789
48.118975	1585.994693	18.744807
48.182336	1584.637803	18.749824
48.456270	1575.700514	18.754842
48.540444	1573.465677	18.759859
48.634077	1574.067153	18.764877
48.431124	1581.362161	18.769895
48.449807	1591.290542	18.774912
48.622545	1572.589601	18.779930
48.317846	1578.310460	18.784947
48.366120	1583.871202	18.789965
48.352850	1577.222134	18.794983
48.315652	1578.625507	18.800000
48.469715	1580.860418	18.805018
48.354900	1588.275084	18.810035
48.649059	1587.935341	18.815053
48.489842	1608.670022	18.820071
48.497847	1611.479596	18.825088
49.078929	1608.051763	18.830106
48.611613	1608.777315	18.835123
49.015633	1598.943848	18.840141
49.192863	1600.413700	18.845159
49.274741	1601.659652	18.850176
49.619791	1602.696098	18.855194
49.016554	1605.799008	18.860211
49.593514	1596.357184	18.865229
49.405563	1595.634997	18.870247
49.194172	1608.354538	18.875264
49.273029	1598.235507	18.880282
49.186790	1610.175294	18.885299
49.481133	1615.690509	18.890317
49.566000	1616.086526	18.895335
49.735609	1627.879338	18.900352
49.991080	1627.301152	18.905370
49.411714	1622.437342	18.910387
49.659915	1618.158080	18.915405
49.948965	1625.562622	18.920423
49.721055	1637.558848	18.925440
49.996777	1627.144122	18.930458
50.085139	1638.184599	18.935475
49.872838	1633.887540	18.940493
49.915771	1636.505925	18.945511
49.816683	1631.126624	18.950528
50.319661	1627.098530	18.955546
50.074555	1632.039097	18.960563
50.088517	1628.276194	18.965581
50.194795	1634.244569	18.970599
50.169506	1632.318201	18.975616
50.095761	1627.780388	18.980634
50.050837	1628.624982	18.985651
50.287607	1636.761484	18.990669
50.491597	1651.647010	18.995687
50.711832	1651.728844	19.000704
50.705593	1652.820536	19.005722
50.476715	1666.281477	19.010739
50.583218	1655.968441	19.015757
50.702399	1655.877622	19.020775
50.470688	1657.688779	19.025792
50.711304	1651.416051	19.030810
50.653162	1662.478339	19.035827
50.903813	1663.074439	19.040845
50.824532	1659.565507	19.045863
50.796246	1662.179525	19.050880
50.812830	1654.443381	19.055898
50.939428	1672.545637	19.060915
51.542469	1664.069416	19.065933
51.417525	1661.074299	19.070951
51.050059	1665.009531	19.075968
51.318071	1663.828426	19.080986
51.562913	1679.359508	19.086003
51.201427	1677.912273	19.091021
51.698972	1683.351060	19.096039
51.402842	1680.981799	19.101056
51.667010	1684.399429	19.106074
51.559592	1684.281828	19.111091
51.719808	1684.558072	19.116109
51.739117	1676.372366	19.121127
51.221089	1679.114836	19.126144
51.705627	1683.415212	19.131162
51.597867	1685.041428	19.136179
51.488312	1684.482132	19.141197
51.605594	1683.590130	19.146215
51.837475	1695.461158	19.151232
52.221064	1709.241323	19.156250
51.891989	1712.641101	19.161267
52.086448	1722.350407	19.166285
52.292994	1712.519257	19.171303
52.307512	1720.176854	19.176320
52.266672	1716.059285	19.181338
52.349105	1709.108591	19.186355
52.391314	1714.051341	19.191373
52.296119	1711.353501	19.196391
52.250469	1713.297017	19.201408
52.147915	1710.713613	19.206426
52.199018	1715.669889	19.211443
52.322176	1718.139422	19.216461
52.685449	1723.462781	19.221479
52.491292	1737.040950	19.226496
52.701829	1734.654582	19.231514
52.786597	1733.975411	19.236531
52.509900	1734.043690	19.241549
52.801468	1730.285250	19.246567
52.552548	1728.733537	19.251584
52.673207	1730.085005	19.256602
52.994237	1750.361818	19.261619
52.918451	1762.403885	19.266637
53.162637	1755.634233	19.271655
53.218420	1765.762105	19.276672
53.367314	1764.802919	19.281690
53.126354	1760.999625	19.286707
53.158667	1761.316721	19.291725
53.259340	1764.744714	19.296743
53.329830	1770.985493	19.301760
53.520185	1759.938534	19.306778
53.556882	1751.160104	19.311795
53.390759	1762.727348	19.316813
53.466868	1758.002779	19.321831
53.464668	1775.048924	19.326848
53.765930	1782.358786	19.331866
53.830510	1785.290724	19.336883
53.869628	1787.561305	19.341901
53.964592	1778.794015	19.346919
54.017728	1786.801793	19.351936
54.039303	1773.956953	19.356954
54.088935	1789.727721	19.361971
54.136667	1793.662050	19.366989
54.381602	1778.403062	19.372007
54.306702	1791.552470	19.377024
54.100030	1784.847634	19.382042
54.118393	1783.001590	19.387059
54.127270	1782.037206	19.392077
54.272189	1780.970897	19.397095
54.470023	1795.381692	19.402112
54.556819	1801.444483	19.407130
54.904384	1806.049900	19.412147
54.689416	1818.044209	19.417165
54.984772	1808.555924	19.422183
54.837001	1809.483788	19.427200
54.927094	1800.740858	19.432218
54.685027	1796.156689	19.437235
54.686004	1802.258338	19.442253
54.706870	1811.334689	19.447271
54.962907	1818.499192	19.452288
54.973385	1808.978474	19.457306
55.077751	1811.718446	19.462323
54.879289	1822.004889	19.467341
55.239313	1810.187542	19.472359
54.780318	1814.212133	19.477376
55.069469	1819.029800	19.482394
55.001079	1828.447602	19.487411
55.276102	1841.183366	19.492429
55.515807	1836.304472	19.497447
55.553431	1838.385740	19.502464
55.919380	1829.856785	19.507482
55.618869	1834.110947	19.512499
55.334384	1834.930836	19.517517
55.709933	1827.798837	19.522535
55.451384	1839.601117	19.527552
55.621902	1836.540750	19.532570
55.625370	1851.131258	19.537587
55.555811	1856.187841	19.542605
55.826108	1868.727745	19.547623
55.944240	1872.687048	19.552640
56.223972	1862.347025	19.557658
56.411439	1861.813499	19.562675
55.942767	1875.588169	19.567693
56.480270	1858.529998	19.572711
56.693784	1860.227696	19.577728
56.611464	1857.638679	19.582746
56.608390	1860.067805	19.587763
56.643484	1856.171691	19.592781
56.465367	1850.343993	19.597799
56.366865	1864.915383	19.602816
56.356675	1848.693372	19.607834
56.424823	1864.617006	19.612851
56.263387	1865.399181	19.617869
56.984846	1884.791945	19.622887
57.051099	1888.872004	19.627904
56.998433	1891.631531	19.632922
57.039429	1898.415857	19.637939
57.458290	1893.115094	19.642957
57.192906	1891.969490	19.647975
57.078946	1889.491699	19.652992
57.023618	1882.796500	19.658010
57.336506	1885.994825	19.663027
57.265281	1878.858548	19.668045
57.245677	1881.804719	19.673063
57.348281	1883.540559	19.678080
57.386422	1881.160426	19.683098
57.384522	1880.583165	19.688115
57.164920	1879.970622	19.693133
57.618408	1879.845362	19.698151
57.329791	1883.241085	19.703168
57.582735	1906.136397	19.708186
57.881949	1909.206340	19.713203
57.714500	1915.417486	19.718221
57.727967	1903.822086	19.723239
57.513961	1918.030472	19.728256
57.869815	1916.222612	19.733274
57.827723	1912.771399	19.738291
57.825548	1916.290554	19.743309
58.353900	1913.109390	19.748327
58.162702	1918.513387	19.753344
58.012329	1931.963625	19.758362
58.517251	1936.076773	19.763379
58.497275	1938.361522	19.768397
58.550664	1936.179520	19.773415
58.685311	1943.324904	19.778432
58.757333	1934.986706	19.783450
59.041395	1937.718494	19.788467
58.712633	1941.842691	19.793485
58.930534	1941.803771	19.798503
58.742849	1943.109263	19.803520
58.761372	1938.567649	19.808538
58.938074	1932.276679	19.813555
58.920151	1937.581472	19.818573
58.810213	1929.008015	19.823591
58.935057	1928.932811	19.828608
58.756135	1926.772916	19.833626
58.795731	1934.452582	19.838643
58.794349	1945.353441	19.843661
58.811683	1943.841041	19.848679
59.118546	1957.400859	19.853696
58.809405	1972.267087	19.858714
59.232243	1964.629590	19.863731
59.432426	1971.814876	19.868749
59.637381	1965.639729	19.873767
59.422851	1965.922261	19.878784
59.447137	1975.950690	19.883802
60.030933	1985.656283	19.888819
59.705526	1993.279357	19.893837
60.094206	1995.703443	19.898855
60.196653	1994.000488	19.903872
59.792105	1989.084287	19.908890
60.301388	1980.471034	19.913907
60.223244	1988.720097	19.918925
60.251187	1983.396700	19.923943
60.631334	1986.489148	19.928960
60.411027	1975.900014	19.933978
60.592264	1967.645058	19.938995
60.001184	1978.002880	19.944013
60.212032	1973.937911	19.949031
60.380571	1987.374305	19.954048
60.038262	1991.171895	19.959066
60.575233	1992.115624	19.964083
60.415051	1982.405707	19.969101
60.495973	1982.656850	19.974119
60.669292	1994.985016	19.979136
60.790760	2011.064696	19.984154
60.902573	2016.020831	19.989171
61.031814	2017.871996	19.994189
60.999265	2015.904261	19.999207
61.112490	2013.815744	20.004224
61.103931	2020.874674	20.009242
61.704845	2008.336016	20.014259
61.491350	2014.402741	20.019277
61.478134	2017.482423	20.024295
61.374322	2016.792414	20.029312
61.540246	2018.251528	20.034330
61.558531	2017.751271	20.039347
61.436519	2020.108938	20.044365
61.539909	2014.526518	20.049383
61.771352	2012.373526	20.054400
61.447817	2018.379147	20.059418
61.727356	2012.030054	20.064435
61.466432	2015.148454	20.069453
61.525590	2007.907158	20.074471
61.772147	2011.060245	20.079488
61.716180	2033.537022	20.084506
61.971780	2034.025377	20.089523
62.094125	2048.780392	20.094541
62.129060	2040.222306	20.099559
62.184586	2034.804037	20.104576
61.889318	2040.902693	20.109594
62.066946	2039.345841	20.114611
62.084986	2040.443915	20.119629
62.194288	2045.527097	20.124647
62.360801	2062.036978	20.129664
62.423570	2067.721443	20.134682
62.564391	2066.745436	20.139699
62.688679	2074.877313	20.144717
62.521669	2063.244499	20.149735
62.823378	2061.327274	20.154752
62.542277	2074.166096	20.159770
62.830524	2075.474351	20.164787
62.647292	2078.610263	20.169805
62.776077	2094.644821	20.174823
63.035994	2094.728984	20.179840
62.855800	2098.166456	20.184858
63.321129	2094.846644	20.189875
63.201976	2102.682287	20.194893
63.152926	2104.867086	20.199911
63.446157	2103.531692	20.204928
63.003221	2100.349656	20.209946
64.033546	2103.141007	20.214963
64.565320	2097.267636	20.219981
64.457111	2079.935427	20.224999
64.210155	2070.468180	20.230016
64.263539	2073.202175	20.235034
64.852994	2068.236748	20.240051
64.690316	2058.620779	20.245069
64.489798	2048.697013	20.250087
64.184110	2043.594341	20.255104
64.005446	2032.447145	20.260122
63.999595	2036.629986	20.265139
64.078574	2031.244160	20.270157
64.240097	2034.472166	20.275175
63.966039	2046.446196	20.280192
64.024941	2062.895372	20.285210
64.217679	2065.430164	20.290227
64.121788	2074.811610	20.295245
64.231455	2067.080065	20.300263
64.570330	2064.043927	20.305280
64.370308	2077.897858	20.310298
64.785951	2095.906563	20.315315
64.840825	2097.610713	20.320333
65.027055	2101.423143	20.325351
64.960307	2094.855518	20.330368
64.872596	2101.653388	20.335386
64.962646	2101.570360	20.340403
65.179524	2098.191066	20.345421
65.333468	2098.187517	20.350439
65.407914	2100.896921	20.355456
65.109261	2101.075673	20.360474
65.342966	2102.863782	20.365491
65.495953	2095.724675	20.370509
65.521741	2107.158545	20.375527
65.339208	2096.963659	20.380544
65.401692	2114.119442	20.385562
65.623178	2116.025126	20.390579
65.604094	2131.673509	20.395597
66.030949	2120.435966	20.400615
66.194727	2117.796641	20.405632
66.076104	2127.278494	20.410650
66.119482	2119.420631	20.415667
65.968002	2125.949451	20.420685
66.149723	2115.746013	20.425703
66.132141	2120.534044	20.430720
65.697559	2118.169486	20.435738
66.118946	2115.217713	20.440755
65.917257	2118.104089	20.445773
66.107402	2140.515824	20.450791
66.504650	2144.705199	20.455808
66.261101	2148.465053	20.460826
66.464965	2146.413189	20.465843
66.782639	2153.433526	20.470861
66.698108	2154.184573	20.475879
66.876151	2138.518997	20.480896
66.552316	2147.411417	20.485914
66.901022	2165.058051	20.490931
67.231930	2170.424493	20.495949
66.842414	2170.907195	20.500967
67.035035	2172.399035	20.505984
66.996775	2175.402514	20.511002
67.066020	2174.957837	20.516019
66.927457	2170.498622	20.521037
66.758309	2180.492757	20.526055
67.356288	2199.422685	20.531072
67.533178	2198.996235	20.536090
67.944439	2197.905511	20.541107
67.830982	2200.784124	20.546125
67.626121	2191.300646	20.551143
67.960031	2192.122609	20.556160
67.942683	2195.328838	20.561178
68.033733	2197.411862	20.566195
67.942141	2196.596404	20.571213
68.007099	2194.062496	20.576231
68.218790	2193.644654	20.581248
68.027343	2201.856061	20.586266
68.304057	2198.583613	20.591283
68.500829	2210.960135	20.596301
68.263392	2221.398589	20.601319
68.762115	2222.703181	20.606336
68.661404	2220.985406	20.611354
68.894382	2225.110548	20.616371
69.172776	2221.747371	20.621389
68.763476	2217.855176	20.626407
68.855080	2204.383690	20.631424
68.908101	2219.936505	20.636442
68.924573	2213.600178	20.641459
68.789923	2222.831372	20.646477
68.588301	2219.476319	20.651495
69.200883	2215.067981	20.656512
69.048120	2218.630104	20.661530
69.050066	2214.678616	20.666547
69.173595	2214.159208	20.671565
68.857545	2217.380043	20.676583
68.992585	2230.081056	20.681600
69.272944	2242.138298	20.686618
69.280653	2246.625013	20.691635
69.350219	2245.694181	20.696653
69.348068	2251.630550	20.701671
69.393640	2253.940290	20.706688
69.756394	2272.389477	20.711706
69.764317	2285.138341	20.716723
69.908274	2279.424284	20.721741
70.255243	2277.639038	20.726759
70.284243	2275.624482	20.731776
70.149384	2279.037461	20.736794
70.331074	2278.703060	20.741811
70.440997	2279.177689	20.746829
70.031835	2278.748741	20.751847
70.270283	2268.458278	20.756864
70.447052	2282.938203	20.761882
70.635239	2289.931277	20.766899
70.886452	2303.227353	20.771917
70.793575	2309.262378	20.776935
71.205774	2307.992158	20.781952
71.292001	2310.029560	20.786970
71.179311	2292.118107	20.791987
71.239970	2271.569178	20.797005
70.742033	2273.186107	20.802023
71.145266	2270.783867	20.807040
71.100989	2293.939567	20.812058
71.224499	2288.545758	20.817075
71.065284	2294.520565	20.822093
71.282370	2296.975218	20.827111
71.519252	2291.514559	20.832128
71.288675	2298.908717	20.837146
71.470805	2293.003722	20.842163
72.052773	2303.111763	20.847181
71.515715	2302.674108	20.852199
71.843120	2310.914521	20.857216
71.558052	2318.695723	20.862234
71.687765	2313.717014	20.867251
72.315620	2324.210252	20.872269
71.905320	2321.818189	20.877287
72.125456	2319.654372	20.882304
72.260902	2318.253668	20.887322
72.206255	2327.687692	20.892339
72.387791	2312.872448	20.897357
72.224503	2333.601728	20.902375
72.646411	2337.252355	20.907392
72.732151	2346.161379	20.912410
72.720928	2343.764659	20.917427
72.650686	2348.617798	20.922445
72.592342	2342.800689	20.927463
72.799344	2343.368386	20.932480
72.847300	2350.653650	20.937498
72.819092	2350.688591	20.942515
72.963192	2338.630741	20.947533
73.055650	2341.040778	20.952551
72.945687	2339.844392	20.957568
73.054813	2343.983028	20.962586
73.567469	2357.320049	20.967603
73.740259	2356.986279	20.972621
73.495514	2371.124495	20.977639
73.623284	2359.278462	20.982656
73.295319	2363.365678	20.987674
73.389331	2370.779685	20.992691
73.734408	2364.517525	20.997709
73.709170	2371.092393	21.002727
73.855665	2362.765672	21.007744
73.893769	2367.806835	21.012762
73.812478	2369.775786	21.017779
73.987609	2379.386360	21.022797
73.731685	2396.969241	21.027815
74.147347	2390.466918	21.032832
74.205242	2399.864948	21.037850
74.301970	2400.712166	21.042867
74.559878	2396.518443	21.047885
74.553505	2396.586084	21.052903
74.598295	2395.177806	21.057920
74.425860	2415.044209	21.062938
74.745890	2419.752539	21.067955
74.985774	2415.884182	21.072973
74.971318	2414.707168	21.077991
75.334712	2415.040696	21.083008
75.072106	2415.759589	21.088026
74.922045	2417.669508	21.093043
75.338187	2415.353284	21.098061
75.061566	2414.004130	21.103079
75.240021	2412.448681	21.108096
75.342012	2411.456034	21.113114
75.696248	2425.665531	21.118131
75.949422	2428.647754	21.123149
75.802797	2417.991485	21.128167
76.043956	2406.062045	21.133184
75.882282	2404.715011	21.138202
75.815915	2406.146712	21.143219
76.167372	2409.851069	21.148237
76.258923	2429.583361	21.153255
76.415193	2418.715175	21.158272
76.425272	2411.028435	21.163290
76.121911	2409.714223	21.168307
76.097102	2413.185194	21.173325
76.492128	2428.148813	21.178343
76.348947	2425.765259	21.183360
76.749197	2430.362476	21.188378
76.564757	2432.843433	21.193395
76.861587	2426.103620	21.198413
76.773942	2422.977329	21.203431
76.927731	2424.455725	21.208448
76.909523	2426.510586	21.213466
76.865107	2420.439519	21.218483
77.147375	2413.686303	21.223501
76.776748	2428.430653	21.228519
77.014414	2416.891119	21.233536
77.075571	2421.349700	21.238554
76.861432	2444.297540	21.243571
77.419036	2447.204473	21.248589
77.368285	2449.504435	21.253607
77.351378	2453.268337	21.258624
77.681053	2443.373799	21.263642
77.478678	2449.724460	21.268659
77.585900	2445.714431	21.273677
77.537106	2453.634216	21.278695
77.899786	2464.873055	21.283712
78.070065	2467.125971	21.288730
77.956510	2481.178871	21.293747
78.548687	2469.732209	21.298765
78.122294	2475.747339	21.303783
78.253598	2469.593953	21.308800
78.390532	2474.534440	21.313818
78.339965	2476.556713	21.318835
78.811582	2471.155302	21.323853
78.420753	2474.800288	21.328871
78.489852	2479.491236	21.333888
78.431026	2473.174671	21.338906
78.493625	2493.846129	21.343923
78.736691	2494.980715	21.348941
78.892710	2491.858026	21.353959
78.672017	2498.975403	21.358976
78.787015	2501.583238	21.363994
79.147090	2515.547265	21.369011
79.426232	2515.990983	21.374029
79.355538	2527.656095	21.379047
79.517976	2534.432363	21.384064
79.388833	2529.171575	21.389082
79.113676	2540.309255	21.394099
79.705853	2528.871986	21.399117
79.639164	2525.881557	21.404135
80.037319	2537.349197	21.409152
79.833753	2545.498228	21.414170
79.616903	2554.149653	21.419187
80.135189	2549.185194	21.424205
80.218766	2563.833646	21.429223
80.224375	2560.465129	21.434240
80.163012	2551.858387	21.439258
79.920893	2555.865892	21.444275
80.278465	2551.549254	21.449293
80.470124	2568.023450	21.454311
80.524535	2565.532849	21.459328
80.861038	2574.743400	21.464346
80.835568	2581.667646	21.469363
81.035160	2567.723954	21.474381
81.002009	2576.473523	21.479399
80.982855	2576.280482	21.484416
81.187754	2570.242745	21.489434
81.194156	2576.711976	21.494451
81.361251	2572.756078	21.499469
81.019139	2576.169141	21.504487
80.828709	2577.906176	21.509504
81.313320	2581.042663	21.514522
81.346778	2586.994727	21.519539
81.684713	2597.718465	21.524557
81.691228	2601.563622	21.529575
81.594622	2603.423351	21.534592
81.707019	2592.804304	21.539610
81.648318	2605.921185	21.544627
81.689841	2605.788474	21.549645
81.799521	2607.870947	21.554663
82.134991	2630.918638	21.559680
82.675863	2630.999690	21.564698
82.050765	2635.095824	21.569715
82.473329	2625.537957	21.574733
82.585670	2626.043677	21.579751
82.420025	2633.153127	21.584768
82.745655	2617.142573	21.589786
82.650827	2624.893596	21.594803
82.500512	2622.268090	21.599821
82.726714	2626.887622	21.604839
83.160295	2646.022912	21.609856
83.278358	2646.446701	21.614874
83.098078	2652.424226	21.619891
83.432829	2643.447487	21.624909
83.384490	2655.582664	21.629927
83.233853	2657.124580	21.634944
83.636514	2647.062520	21.639962
83.254608	2651.883657	21.644979
83.405044	2643.734705	21.649997
83.711681	2647.918228	21.655015
83.458367	2656.612499	21.660032
83.346433	2664.521230	21.665050
83.380068	2688.605898	21.670067
83.997741	2686.405374	21.675085
83.962272	2690.079479	21.680103
84.107938	2683.025421	21.685120
84.629719	2691.193364	21.690138
84.425058	2699.764271	21.695155
84.399669	2702.885367	21.700173
84.759597	2708.511681	21.705191
84.869667	2705.102087	21.710208
84.810324	2705.696544	21.715226
84.659568	2713.549352	21.720243
85.154137	2707.753257	21.725261
84.946567	2708.463385	21.730279
84.754456	2707.831473	21.735296
85.066708	2704.738885	21.740314
85.005377	2709.572630	21.745331
84.837800	2701.206132	21.750349
84.822310	2707.727682	21.755367
85.275225	2729.473073	21.760384
85.340579	2726.351421	21.765402
84.990726	2743.930033	21.770419
85.168917	2735.436792	21.775437
85.613521	2742.791145	21.780455
85.710955	2756.075191	21.785472
86.250524	2749.567896	21.790490
86.119674	2754.242838	21.795507
86.481540	2755.712470	21.800525
86.351968	2759.677696	21.805543
85.848998	2757.791174	21.810560
86.485107	2754.661087	21.815578
86.416635	2756.819189	21.820595
86.454260	2747.874039	21.825613
86.530708	2747.571357	21.830631
86.429255	2754.316659	21.835648
86.734494	2758.175572	21.840666
86.466838	2762.832217	21.845683
87.082878	2770.487256	21.850701
86.751357	2770.097821	21.855719
87.102830	2778.731111	21.860736
87.348865	2774.164753	21.865754
87.323160	2785.123607	21.870771
87.697627	2774.866947	21.875789
87.721900	2771.433264	21.880807
87.477580	2770.167022	21.885824
87.400372	2769.615895	21.890842
87.675936	2775.508188	21.895859
87.784051	2782.424597	21.900877
87.800522	2784.678494	21.905895
87.623446	2778.432570	21.910912
87.976189	2786.372667	21.915930
87.774647	2802.476417	21.920947
87.907994	2796.921173	21.925965
87.977866	2802.902915	21.930983
87.933490	2809.031096	21.936000
88.552206	2815.097582	21.941018
88.562316	2822.082342	21.946035
88.891650	2832.374208	21.951053
88.816324	2825.290822	21.956071
88.773089	2826.010145	21.961088
89.099294	2823.871817	21.966106
88.701593	2824.387303	21.971123
89.033409	2823.559348	21.976141
89.364108	2818.292770	21.981159
89.185247	2829.468013	21.986176
89.483421	2819.508239	21.991194
89.647545	2828.657558	21.996211
89.336270	2822.115228	22.001229
89.641643	2812.288034	22.006247
89.242593	2822.205999	22.011264
89.817618	2828.239341	22.016282
89.854952	2844.270433	22.021299
90.094056	2855.119461	22.026317
90.291393	2837.254647	22.031335
90.289220	2848.131136	22.036352
90.409704	2851.029203	22.041370
90.330900	2849.214254	22.046387
90.238505	2853.270328	22.051405
90.206304	2840.950710	22.056423
89.985089	2850.057662	22.061440
90.411849	2842.767555	22.066458
90.361896	2853.663466	22.071475
90.174285	2874.413909	22.076493
90.893121	2872.319151	22.081511
90.433867	2878.996500	22.086528
90.608740	2868.180865	22.091546
90.955819	2882.261375	22.096563
91.079128	2895.601991	22.101581
91.246284	2898.933912	22.106599
91.177946	2899.659601	22.111616
91.289641	2896.250490	22.116634
91.182901	2895.054330	22.121651
91.524156	2911.827568	22.126669
91.979989	2912.016580	22.131687
91.831551	2918.796981	22.136704
92.066466	2916.373501	22.141722
92.020533	2917.498361	22.146739
91.906909	2914.465780	22.151757
92.033799	2917.474538	22.156775
91.893945	2921.062302	22.161792
92.254760	2922.923065	22.166810
92.441390	2932.326080	22.171827
92.659122	2939.991241	22.176845
92.918844	2939.237706	22.181863
92.623802	2947.340978	22.186880
92.788174	2941.400799	22.191898
93.241672	2947.587297	22.196915
93.321387	2939.886027	22.201933
93.249569	2939.750149	22.206951
92.740889	2946.473167	22.211968
93.112626	2944.056968	22.216986
92.961334	2945.347302	22.222003
93.137045	2967.614729	22.227021
93.422407	2969.721154	22.232039
93.384491	2975.871973	22.237056
93.573050	2977.447929	22.242074
93.531892	2982.377660	22.247091
93.638083	2978.723985	22.252109
94.174770	2996.261418	22.257127
93.842190	3003.580949	22.262144
94.230317	2997.189733	22.267162
94.337173	2998.661515	22.272179
94.366611	3000.897645	22.277197
94.256346	2997.678870	22.282215
94.473619	3010.951904	22.287232
94.469337	3026.251201	22.292250
94.445829	3026.518231	22.297267
94.641566	3028.261383	22.302285
94.888002	3029.242874	22.307303
94.773435	3028.861310	22.312320
94.932594	3027.143686	22.317338
95.186879	3024.820146	22.322355
95.259414	3042.721129	22.327373
95.424539	3050.366419	22.332391
95.483904	3055.100009	22.337408
95.723779	3048.851978	22.342426
95.734530	3047.506490	22.347443
95.745896	3044.004006	22.352461
96.033336	3038.064614	22.357479
96.003988	3048.405967	22.362496
96.377296	3039.944365	22.367514
96.281190	3038.576587	22.372531
95.942722	3047.449856	22.377549
96.384943	3032.710306	22.382567
96.110567	3042.610896	22.387584
96.341091	3045.625965	22.392602
96.333814	3061.781615	22.397619
96.529322	3068.782551	22.402637
96.796782	3073.490828	22.407655
96.786739	3077.891742	22.412672
96.932785	3071.510781	22.417690
97.171013	3071.442664	22.422707
97.032280	3063.510289	22.427725
97.209372	3076.334340	22.432743
97.287948	3091.216957	22.437760
97.557498	3093.988255	22.442778
97.544334	3090.849155	22.447795
97.698376	3094.437290	22.452813
97.805118	3091.179955	22.457831
97.720461	3101.905383	22.462848
97.812130	3089.591760	22.467866
97.951193	3092.565575	22.472883
97.687401	3093.785761	22.477901
97.879461	3106.013554	22.482919
97.648063	3119.488815	22.487936
98.022998	3119.608925	22.492954
98.512504	3125.242270	22.497971
98.745482	3142.947094	22.502989
98.818242	3145.789115	22.508007
99.046963	3158.903133	22.513024
98.990828	3143.586904	22.518042
99.310651	3146.250294	22.523059
99.178858	3147.428195	22.528077
99.301400	3147.221990	22.533095
98.865456	3145.522166	22.538112
99.310714	3149.505955	22.543130
99.445430	3151.708800	22.548147
99.278402	3147.389123	22.553165
99.398666	3160.448069	22.558183
99.430166	3176.736107	22.563200
99.478421	3173.771265	22.568218
99.663064	3177.614126	22.573235
99.435485	3179.164431	22.578253
99.692997	3186.686506	22.583271
99.825777	3204.091160	22.588288
100.020886	3203.118223	22.593306
100.246019	3202.043743	22.598323
100.465012	3201.685283	22.603341
100.567325	3221.090480	22.608359
100.751043	3231.243806	22.613376
100.748831	3222.552506	22.618394
100.889029	3226.265594	22.623411
100.893705	3226.765694	22.628429
101.036739	3226.182573	22.633447
101.187195	3221.715489	22.638464
101.099568	3227.124687	22.643482
101.283789	3230.383167	22.648499
101.490407	3247.551123	22.653517
101.633250	3247.258296	22.658535
101.528698	3252.547489	22.663552
101.724082	3259.749127	22.668570
101.975211	3245.054785	22.673587
102.085043	3245.707240	22.678605
102.040901	3244.114048	22.683623
101.980071	3246.951434	22.688640
102.232615	3257.101669	22.693658
102.400758	3273.682675	22.698675
102.034710	3269.113086	22.703693
102.703298	3259.832589	22.708711
102.624002	3266.111269	22.713728
102.492949	3273.522295	22.718746
103.169468	3259.589207	22.723763
102.841975	3270.207170	22.728781
102.932630	3272.929155	22.733799
103.439278	3285.742526	22.738816
103.378213	3286.479661	22.743834
103.313593	3286.470852	22.748851
103.404943	3297.954197	22.753869
103.691441	3283.653783	22.758887
103.957334	3282.170831	22.763904
103.624603	3279.866920	22.768922
104.178332	3283.916045	22.773939
103.961743	3287.204630	22.778957
103.974109	3299.362912	22.783975
104.132891	3309.274841	22.788992
104.252640	3310.853941	22.794010
104.379962	3307.092980	22.799027
103.874711	3322.050056	22.804045
104.536182	3317.432228	22.809063
104.669477	3325.477628	22.814080
104.711976	3339.824263	22.819098
105.028579	3330.214404	22.824115
105.147919	3336.094081	22.829133
105.251363	3339.070481	22.834151
105.299255	3329.298950	22.839168
105.353099	3331.364473	22.844186
105.367165	3326.225299	22.849203
105.193442	3336.943863	22.854221
105.644703	3333.091906	22.859239
105.916057	3342.970174	22.864256
105.998353	3353.452838	22.869274
106.111099	3355.831491	22.874291
106.384355	3359.150532	22.879309
106.274344	3354.303309	22.884327
106.203074	3360.686945	22.889344
105.960680	3361.357030	22.894362
106.375663	3351.134415	22.899379
106.241812	3351.738420	22.904397
106.473725	3351.449480	22.909415
106.523591	3364.450612	22.914432
106.460925	3384.787749	22.919450
106.880016	3381.839245	22.924467
107.044142	3382.432705	22.929485
107.223066	3375.327387	22.934503
107.174286	3381.985126	22.939520
107.098468	3386.671158	22.944538
107.403994	3399.987110	22.949555
107.425733	3415.119044	22.954573
107.364857	3415.568247	22.959591
107.721630	3418.713510	22.964608
107.642150	3416.678338	22.969626
107.697040	3430.656515	22.974643
107.947999	3439.545366	22.979661
107.889688	3444.695100	22.984679
108.106626	3440.110365	22.989696
108.346593	3434.985474	22.994714
108.640502	3449.957620	22.999731
108.932189	3464.616268	23.004749
109.277212	3461.035304	23.009767
109.468453	3453.675473	23.014784
109.394370	3449.595754	23.019802
109.426826	3426.408961	23.024819
109.230199	3423.975553	23.029837
109.798563	3434.104654	23.034855
109.667246	3427.183299	23.039872
109.485440	3437.872547	23.044890
109.955729	3438.337736	23.049907
109.540734	3446.555592	23.054925
109.857580	3457.450885	23.059943
109.982589	3452.295548	23.064960
109.677974	3463.803622	23.069978
109.875601	3455.356425	23.074995
110.044330	3452.662584	23.080013
110.138208	3473.819730	23.085031
110.205660	3479.806856	23.090048
110.296548	3483.411452	23.095066
110.363800	3473.753159	23.100083
110.412285	3494.982865	23.105101
110.542135	3507.031335	23.110119
111.227166	3499.894808	23.115136
111.160944	3504.759487	23.120154
111.282115	3498.059786	23.125171
111.081467	3499.261281	23.130189
111.555105	3489.753712	23.135207
111.580961	3503.558022	23.140224
111.569039	3519.393182	23.145242
111.817826	3514.409239	23.150259
111.518558	3522.715666	23.155277
111.806373	3524.850103	23.160295
112.278613	3526.052067	23.165312
111.908849	3528.298446	23.170330
111.984070	3512.702078	23.175347
112.049952	3538.246154	23.180365
112.454496	3546.323152	23.185383
112.718155	3547.026609	23.190400
112.429769	3551.112556	23.195418
113.012681	3549.036242	23.200435
112.939665	3549.472438	23.205453
112.861448	3549.199125	23.210471
113.216297	3563.870613	23.215488
113.130564	3570.078865	23.220506
113.369345	3577.806298	23.225523
113.681309	3585.071318	23.230541
113.350501	3576.134069	23.235559
113.738438	3577.482424	23.240576
113.757155	3573.885817	23.245594
113.873611	3586.601989	23.250611
114.159641	3598.809704	23.255629
113.893688	3606.934658	23.260647
114.529474	3599.596689	23.265664
114.405400	3598.870501	23.270682
114.225229	3592.350180	23.275699
114.324099	3602.267143	23.280717
114.634664	3622.696915	23.285735
114.797890	3630.805361	23.290752
114.789890	3629.655539	23.295770
115.112859	3630.066350	23.300787
115.109444	3630.557527	23.305805
115.265129	3647.638106	23.310823
115.741742	3649.596139	23.315840
115.881612	3646.470275	23.320858
115.860773	3641.463208	23.325875
116.229081	3639.436050	23.330893
116.220987	3638.427838	23.335911
116.627344	3632.736706	23.340928
116.150489	3645.084992	23.345946
116.529997	3639.585361	23.350963
116.710326	3632.825820	23.355981
116.519992	3636.790744	23.360999
116.814044	3630.718691	23.366016
116.865257	3630.643425	23.371034
116.912088	3632.300267	23.376051
116.962838	3635.380315	23.381069
117.156584	3640.192570	23.386087
117.077370	3629.158086	23.391104
116.811053	3629.235719	23.396122
117.346747	3637.387038	23.401139
117.462633	3647.291091	23.406157
117.452762	3651.429410	23.411175
117.858006	3654.793552	23.416192
117.653028	3658.858361	23.421210
117.589841	3654.212033	23.426227
117.738241	3659.023659	23.431245
117.680369	3663.503175	23.436263
118.327657	3669.439609	23.441280
118.007193	3677.939085	23.446298
118.088193	3678.130463	23.451315
118.367251	3684.964977	23.456333
118.399216	3706.693213	23.461351
118.683147	3712.281695	23.466368
118.865742	3714.362928	23.471386
118.754969	3711.881167	23.476403
118.852298	3716.777261	23.481421
119.096858	3735.395833	23.486439
119.639690	3733.973302	23.491456
118.996245	3731.241365	23.496474
119.465930	3726.539934	23.501491
119.568748	3740.299155	23.506509
119.502808	3760.680601	23.511527
119.947147	3758.804141	23.516544
120.314645	3759.250336	23.521562
120.213426	3759.467625	23.526579
120.288740	3756.005906	23.531597
120.155931	3768.506322	23.536615
120.612539	3768.902122	23.541632
120.569739	3788.576648	23.546650
120.744582	3785.229635	23.551667
120.649374	3775.113258	23.556685
120.536881	3791.185012	23.561703
121.149083	3799.999173	23.566720
121.258835	3814.296217	23.571738
121.453037	3814.746448	23.576755
121.527237	3816.654610	23.581773
121.490898	3810.591117	23.586791
121.815446	3814.769767	23.591808
121.959871	3845.242843	23.596826
121.796226	3838.206089	23.601843
122.349681	3839.109575	23.606861
122.208524	3848.303495	23.611879
122.298526	3843.447815	23.616896
122.346299	3843.679893	23.621914
122.544760	3851.177117	23.626931
122.719864	3858.481405	23.631949
122.962099	3868.365460	23.636967
123.330096	3854.570692	23.641984
123.157353	3858.860907	23.647002
123.264434	3856.349889	23.652019
123.327197	3848.594207	23.657037
123.551342	3858.894923	23.662055
123.810746	3874.669894	23.667072
124.002622	3878.650241	23.672090
124.065279	3875.963798	23.677107
124.273907	3880.330084	23.682125
123.884863	3889.649304	23.687143
124.201419	3880.179908	23.692160
124.069530	3886.372840	23.697178
124.353342	3884.798868	23.702195
124.671287	3868.318545	23.707213
124.553747	3884.671256	23.712231
124.514118	3877.455802	23.717248
124.729630	3899.613678	23.722266
124.852442	3907.624097	23.727283
124.903993	3910.723742	23.732301
124.970933	3911.364189	23.737319
125.369245	3905.634117	23.742336
125.301552	3924.987904	23.747354
125.433769	3940.835934	23.752371
125.579576	3938.547646	23.757389
125.507548	3938.702856	23.762407
125.746942	3936.947949	23.767424
125.872760	3961.265451	23.772442
125.810752	3970.779585	23.777459
126.216377	3955.200075	23.782477
126.246724	3964.660145	23.787495
126.912598	3976.858741	23.792512
126.886358	3988.619406	23.797530
126.864537	3992.459220	23.802547
127.156948	3992.589357	23.807565
127.014553	3986.473476	23.812583
127.409338	3986.097983	23.817600
127.105524	3992.649560	23.822618
127.469678	4006.782719	23.827635
127.568752	4005.364059	23.832653
127.982366	4013.273099	23.837671
128.355421	4002.878935	23.842688
128.077568	4013.039542	23.847706
127.996867	4015.288670	23.852723
128.194301	4009.631497	23.857741
127.916454	4023.463485	23.862759
128.151537	4033.155272	23.867776
128.635628	4044.716604	23.872794
128.595630	4040.512497	23.877811
128.525507	4045.139616	23.882829
128.560947	4049.337689	23.887847
129.067711	4057.224819	23.892864
129.063966	4063.123630	23.897882
129.288277	4067.053229	23.902899
129.677035	4081.955047	23.907917
129.682075	4085.587642	23.912935
129.559035	4086.953021	23.917952
129.802596	4093.621107	23.922970
130.109905	4089.595246	23.927987
130.561194	4079.698317	23.933005
130.346864	4096.676368	23.938023
130.198328	4104.767924	23.943040
130.517900	4118.974381	23.948058
130.598796	4120.561339	23.953075
130.739674	4114.707036	23.958093
130.835565	4110.753429	23.963111
130.797066	4114.093250	23.968128
131.002565	4119.535489	23.973146
131.288856	4136.315756	23.978163
131.684070	4132.854858	23.983181
131.665941	4131.098513	23.988199
131.830201	4133.993004	23.993216
131.747305	4132.202932	23.998234
131.670936	4129.114596	24.003251
132.257648	4121.412890	24.008269
131.974256	4131.362846	24.013287
132.204625	4148.209472	24.018304
132.307390	4153.476156	24.023322
132.278507	4155.742216	24.028339
132.531371	4161.821205	24.033357
132.111082	4179.179116	24.038375
132.506948	4188.231761	24.043392
133.003891	4190.162244	24.048410
133.061919	4189.587922	24.053427
133.596168	4206.168249	24.058445
133.506029	4215.350329	24.063463
133.719514	4208.700880	24.068480
133.798511	4210.712957	24.073498
133.891202	4206.703193	24.078515
134.088609	4199.873803	24.083533
133.757629	4211.977456	24.088551
134.401631	4219.335385	24.093568
134.609265	4221.551941	24.098586
134.532355	4231.551640	24.103603
134.832134	4216.864306	24.108621
134.757170	4220.232780	24.113639
134.799213	4227.927423	24.118656
135.067041	4232.200987	24.123674
135.102285	4251.424722	24.128691
135.597462	4247.455397	24.133709
135.590549	4250.792574	24.138727
135.264983	4253.459963	24.143744
135.918431	4257.561910	24.148762
136.008491	4277.174998	24.153779
136.128337	4279.879931	24.158797
136.421114	4277.034786	24.163815
136.572992	4279.065145	24.168832
136.497603	4281.848410	24.173850
136.672623	4279.494051	24.178867
136.716896	4273.993362	24.183885
136.904924	4278.925530	24.188903
136.919708	4277.611540	24.193920
137.377659	4283.425806	24.198938
137.544941	4302.612820	24.203955
137.620910	4295.720935	24.208973
137.611851	4302.308249	24.213991
137.688376	4305.616400	24.219008
137.904526	4308.436571	24.224026
137.800326	4308.242907	24.229043
137.955001	4287.629746	24.234061
137.980292	4302.301034	24.239079
138.022610	4320.625340	24.244096
138.156388	4324.312987	24.249114
138.225237	4329.435673	24.254131
138.570532	4324.333803	24.259149
138.206828	4345.506956	24.264167
138.752037	4354.104002	24.269184
139.185031	4359.701220	24.274202
138.711960	4369.873532	24.279219
139.221706	4374.529441	24.284237
139.194791	4397.127149	24.289255
139.128304	4391.329402	24.294272
139.335454	4389.383700	24.299290
139.489083	4409.627192	24.304307
139.987972	4411.104263	24.309325
140.066899	4418.138599	24.314343
140.322108	4417.006534	24.319360
140.270312	4433.125951	24.324378
140.388090	4453.696189	24.329395
140.857039	4439.186200	24.334413
140.698122	4448.262174	24.339431
140.809280	4444.505077	24.344448
141.220828	4448.246800	24.349466
140.945921	4455.128314	24.354483
141.216093	4455.870117	24.359501
141.449108	4462.598270	24.364519
141.630687	4469.950606	24.369536
141.971860	4483.379082	24.374554
141.946032	4499.421269	24.379571
142.037753	4485.844614	24.384589
142.247107	4486.702319	24.389607
142.332060	4493.199207	24.394624
142.724436	4498.998842	24.399642
142.722521	4515.623320	24.404659
142.910838	4516.449767	24.409677
142.653787	4515.907580	24.414695
142.772851	4508.762488	24.419712
142.990111	4535.685264	24.424730
143.413288	4550.043187	24.429747
143.613460	4537.817254	24.434765
144.123525	4545.701766	24.439783
143.829482	4537.391353	24.444800
144.206010	4530.394004	24.449818
144.125949	4554.976606	24.454835
144.821856	4559.857781	24.459853
144.300241	4571.145639	24.464871
144.722103	4565.413134	24.469888
144.691539	4561.632190	24.474906
144.740422	4568.787033	24.479923
145.059477	4559.290059	24.484941
145.167566	4570.004704	24.489959
145.150051	4591.859357	24.494976
145.304446	4591.319217	24.499994
145.491503	4600.196940	24.505011
145.773467	4591.677432	24.510029
145.382012	4595.962611	24.515047
145.185863	4601.311734	24.520064
145.831637	4618.344407	24.525082
145.677471	4631.259617	24.530099
146.192335	4630.658065	24.535117
146.430947	4643.647542	24.540135
146.401688	4661.206425	24.545152
146.781196	4650.933506	24.550170
146.988132	4648.101979	24.555187
147.186832	4654.069445	24.560205
147.561058	4668.982834	24.565223
147.695635	4675.157995	24.570240
147.946890	4666.539496	24.575258
147.545573	4674.712579	24.580275
147.576098	4664.276593	24.585293
147.912149	4669.536947	24.590311
147.938933	4673.360535	24.595328
148.161931	4683.012199	24.600346
148.503208	4692.629276	24.605363
148.642421	4693.008850	24.610381
148.906923	4709.729526	24.615399
148.607388	4699.904704	24.620416
148.955946	4708.309106	24.625434
149.089259	4724.991716	24.630451
149.478720	4719.285560	24.635469
149.560111	4722.595389	24.640487
149.573607	4725.690260	24.645504
149.863528	4717.400703	24.650522
149.560121	4725.711609	24.655539
149.980961	4737.507004	24.660557
150.275516	4751.651195	24.665575
150.171086	4749.335027	24.670592
150.619511	4747.565579	24.675610
150.244515	4751.435157	24.680627
150.494059	4756.462310	24.685645
150.579579	4770.700427	24.690663
150.475345	4775.449646	24.695680
150.991443	4795.099339	24.700698
151.191214	4804.361433	24.705715
151.650993	4785.394286	24.710733
151.670884	4805.799683	24.715751
151.914622	4820.854400	24.720768
152.462707	4819.047812	24.725786
152.036215	4824.844405	24.730803
152.393162	4821.778875	24.735821
152.639643	4828.999891	24.740839
152.498403	4830.908709	24.745856
152.961650	4818.966296	24.750874
152.667999	4834.575593	24.755891
152.964666	4843.074099	24.760909
153.175543	4851.469069	24.765927
153.196166	4848.674293	24.770944
153.495059	4839.076509	24.775962
153.506542	4853.811126	24.780979
153.805377	4856.574165	24.785997
154.079526	4863.604335	24.791015
153.642184	4868.650578	24.796032
153.982024	4866.967661	24.801050
154.022194	4871.375268	24.806067
154.152848	4877.367049	24.811085
154.546201	4891.560920	24.816103
154.392806	4898.382354	24.821120
154.527455	4899.550163	24.826138
154.852686	4915.096266	24.831155
155.023563	4919.055073	24.836173
155.407687	4919.008538	24.841191
155.418332	4931.333657	24.846208
155.760844	4942.790831	24.851226
155.594309	4940.065215	24.856243
155.781360	4939.156393	24.861261
155.875033	4953.319436	24.866279
156.099580	4964.328126	24.871296
156.644313	4960.262604	24.876314
156.970223	4969.879167	24.881331
156.815255	4966.807906	24.886349
157.202143	4961.353032	24.891367
156.968819	4984.955363	24.896384
157.255276	4981.939590	24.901402
157.642912	4996.217866	24.906419
157.627376	4995.436536	24.911437
157.623569	4992.839161	24.916455
157.622281	5003.606964	24.921472
158.088072	5005.020935	24.926490
158.431033	5018.262379	24.931507
158.322031	5025.319104	24.936525
158.529681	5020.207476	24.941543
158.564496	5022.911944	24.946560
158.688038	5037.233156	24.951578
159.043353	5057.533495	24.956595
159.200103	5052.223064	24.961613
159.215537	5051.155933	24.966631
159.265890	5059.774872	24.971648
159.698834	5075.371629	24.976666
159.945395	5075.129107	24.981683
159.763305	5083.689928	24.986701
160.009428	5073.064292	24.991719
159.950292	5089.249322	24.996736
160.077543	5096.725498	25.001754
160.290695	5105.373577	25.006771
160.422464	5110.915269	25.011789
160.901599	5130.173223	25.016807
161.021934	5135.855211	25.021824
161.587399	5124.956763	25.026842
161.511783	5129.290074	25.031859
161.615323	5134.647462	25.036877
161.762158	5136.999731	25.041895
161.747210	5152.510640	25.046912
162.459538	5152.294554	25.051930
162.155370	5162.940046	25.056947
162.224117	5155.964731	25.061965
162.073695	5149.678136	25.066983
162.263596	5159.193781	25.072000
162.617372	5175.705646	25.077018
162.992870	5181.398892	25.082035
162.637831	5188.115720	25.087053
163.201692	5187.022500	25.092071
163.340313	5206.732933	25.097088
163.483986	5213.880057	25.102106
163.450793	5214.075504	25.107123
163.968682	5216.363116	25.112141
163.749641	5209.715312	25.117159
163.915336	5230.136598	25.122176
164.365887	5238.720155	25.127194
164.596866	5233.869076	25.132211
164.410948	5238.401742	25.137229
164.772421	5251.852076	25.142247
164.918760	5261.098589	25.147264
165.384545	5261.334062	25.152282
165.364248	5272.675475	25.157299
165.313519	5268.755951	25.162317
165.931792	5276.064241	25.167335
165.461811	5283.861530	25.172352
165.563610	5285.724574	25.177370
165.877716	5293.622644	25.182387
165.994956	5311.365853	25.187405
166.181963	5315.457514	25.192423
166.157144	5321.375137	25.197440
166.741775	5334.248692	25.202458
166.615045	5333.787966	25.207475
166.935604	5350.324206	25.212493
167.589538	5362.528235	25.217511
167.525387	5377.716009	25.222528
168.076342	5371.660507	25.227546
168.112084	5370.511441	25.232563
167.594871	5372.533772	25.237581
168.405548	5379.234757	25.242599
168.542900	5387.375839	25.247616
168.754145	5381.751347	25.252634
168.860818	5393.417200	25.257651
168.627746	5389.603818	25.262669
169.184990	5381.391641	25.267687
168.891638	5405.085247	25.272704
169.216555	5415.027186	25.277722
169.570039	5407.462715	25.282739
169.659063	5407.819628	25.287757
170.094218	5413.985727	25.292775
169.800986	5430.129780	25.297792
170.293850	5428.641120	25.302810
170.484211	5438.706019	25.307827
170.257077	5440.621529	25.312845
170.777422	5445.366574	25.317863
170.816597	5464.791885	25.322880
170.824722	5473.574361	25.327898
171.202420	5468.606191	25.332915
171.262896	5469.258754	25.337933
171.240123	5468.394370	25.342951
171.419615	5491.248007	25.347968
171.923492	5492.721258	25.352986
171.877726	5492.324719	25.358003
172.089701	5495.422724	25.363021
172.687457	5487.223699	25.368039
172.337074	5510.167356	25.373056
172.269183	5523.654928	25.378074
172.956900	5523.991916	25.383091
172.760458	5529.722991	25.388109
172.908534	5532.669908	25.393127
172.927530	5549.530602	25.398144
173.249508	5547.983421	25.403162
173.519103	5561.978172	25.408179
173.451287	5577.805576	25.413197
173.938633	5567.514046	25.418215
174.049373	5584.072201	25.423232
174.330437	5602.786455	25.428250
174.598807	5608.821092	25.433267
174.593679	5610.679984	25.438285
174.623813	5604.527263	25.443303
174.800433	5620.693381	25.448320
175.072440	5634.721646	25.453338
175.258110	5632.266247	25.458355
175.193146	5646.226304	25.463373
175.737236	5657.987057	25.468391
175.890795	5658.770336	25.473408
176.304034	5657.665698	25.478426
176.104792	5661.494897	25.483443
176.227876	5683.902295	25.488461
176.755402	5690.079746	25.493479
176.840541	5681.601226	25.498496
177.030089	5685.550183	25.503514
177.208207	5695.768268	25.508531
177.246979	5702.306883	25.513549
177.773363	5700.399806	25.518567
177.727718	5701.045696	25.523584
177.985016	5710.363705	25.528602
178.072376	5719.389390	25.533619
178.454563	5727.291788	25.538637
178.645492	5727.923563	25.543655
178.308981	5734.736026	25.548672
178.624216	5733.606098	25.553690
178.847675	5747.554881	25.558707
178.910194	5759.848031	25.563725
178.825625	5753.182473	25.568743
179.070012	5782.066171	25.573760
179.372274	5785.865796	25.578778
179.593241	5786.406240	25.583795
179.665940	5802.915633	25.588813
179.731847	5810.077807	25.593831
180.136969	5818.836530	25.598848
180.543220	5836.934755	25.603866
180.794446	5841.959656	25.608883
180.704178	5853.746964	25.613901
180.904771	5832.376115	25.618919
181.071333	5847.836785	25.623936
181.349226	5864.016133	25.628954
181.332075	5866.905277	25.633971
181.409613	5876.084470	25.638989
181.637343	5868.838000	25.644007
181.947492	5895.067901	25.649024
182.393205	5906.169493	25.654042
182.610467	5902.510765	25.659059
182.390056	5905.253727	25.664077
182.584371	5914.267987	25.669095
182.769167	5919.290917	25.674112
182.687533	5925.359458	25.679130
183.104004	5941.488474	25.684148
183.610982	5955.520495	25.689165
184.092365	5954.321575	25.694183
183.967480	5947.356304	25.699200
184.176372	5951.473765	25.704218
184.491229	5960.759152	25.709236
184.270176	5973.064647	25.714253
184.673117	5980.240043	25.719271
184.854118	5975.059169	25.724288
184.884629	5980.613400	25.729306
184.832548	5993.462380	25.734324
184.853238	6012.670275	25.739341
185.207428	6020.058812	25.744359
185.553731	6034.487883	25.749376
185.264559	6051.795604	25.754394
185.851823	6053.449168	25.759412
185.768771	6071.484074	25.764429
186.056170	6069.592240	25.769447
186.522768	6087.126474	25.774464
186.925914	6096.457666	25.779482
187.067196	6090.083247	25.784500
187.115251	6109.566998	25.789517
187.847939	6113.088801	25.794535
187.814204	6123.917668	25.799552
188.133530	6131.357453	25.804570
188.238283	6120.178473	25.809588
187.981815	6133.346549	25.814605
188.140022	6124.653136	25.819623
188.617046	6144.815982	25.824640
188.741672	6136.673156	25.829658
188.742583	6145.339951	25.834676
188.806242	6163.279981	25.839693
189.281519	6165.225213	25.844711
189.160353	6169.803698	25.849728
189.448327	6185.468024	25.854746
190.023094	6186.443030	25.859764
189.896039	6201.171180	25.864781
190.071244	6202.328695	25.869799
190.266056	6215.518522	25.874816
190.421518	6230.631243	25.879834
190.334758	6239.548892	25.884852
189.934332	6243.718734	25.889869
190.472084	6256.585627	25.894887
191.009935	6271.761737	25.899904
191.115807	6292.037460	25.904922
191.709200	6281.989747	25.909940
191.707401	6298.446267	25.914957
191.641397	6306.605330	25.919975
191.963157	6314.054261	25.924992
192.567346	6312.207879	25.930010
192.571049	6319.099333	25.935028
192.856825	6334.422700	25.940045
193.249199	6335.552683	25.945063
193.643242	6343.976741	25.950080
193.352782	6337.427145	25.955098
193.694422	6336.858668	25.960116
193.612107	6353.771049	25.965133
193.877693	6359.175432	25.970151
194.239758	6364.492838	25.975168
194.401463	6361.560412	25.980186
194.470294	6365.531159	25.985204
194.353474	6395.438251	25.990221
194.742333	6394.534938	25.995239
194.993144	6400.231232	26.000256
194.932469	6424.867353	26.005274
195.220153	6421.348337	26.010292
195.970389	6431.500110	26.015309
196.127872	6444.788934	26.020327
195.996176	6444.443836	26.025344
195.925449	6449.934130	26.030362
196.485355	6453.826609	26.035380
196.345554	6475.583163	26.040397
196.926420	6477.185085	26.045415
196.947291	6478.936083	26.050432
196.877482	6497.767996	26.055450
197.476964	6499.404718	26.060468
197.834685	6510.091991	26.065485
197.453864	6513.986548	26.070503
198.033275	6523.939808	26.075520
198.139688	6536.040133	26.080538
198.390874	6538.722185	26.085556
198.723505	6565.330504	26.090573
199.017579	6570.556540	26.095591
199.449329	6559.934869	26.100608
198.942951	6573.589294	26.105626
199.515423	6576.877899	26.110644
199.475272	6583.920452	26.115661
199.474608	6581.469429	26.120679
200.001200	6602.713149	26.125696
200.123625	6618.791436	26.130714
200.501960	6619.127434	26.135732
200.474271	6623.248183	26.140749
200.366099	6641.272836	26.145767
200.703000	6641.773589	26.150784
200.597257	6656.118764	26.155802
201.082343	6670.277701	26.160820
201.442306	6678.810457	26.165837
201.601507	6687.051846	26.170855
201.645817	6682.755649	26.175872
202.253520	6698.980897	26.180890
202.602799	6696.697518	26.185908
202.511494	6710.034900	26.190925
202.586707	6709.253960	26.195943
202.897493	6724.777529	26.200960
203.064150	6731.547991	26.205978
203.375191	6728.271453	26.210996
203.487994	6740.517273	26.216013
203.577350	6755.141443	26.221031
203.537949	6761.045443	26.226048
203.808738	6780.697563	26.231066
204.245104	6788.890101	26.236084
204.233906	6801.172263	26.241101
204.507279	6805.861929	26.246119
205.192802	6812.242848	26.251136
204.868929	6831.723111	26.256154
205.187957	6832.313270	26.261172
205.653433	6840.605056	26.266189
205.388715	6846.578057	26.271207
205.728436	6853.877264	26.276224
205.966493	6876.475857	26.281242
206.183342	6871.047404	26.286260
206.362704	6899.091525	26.291277
206.659891	6911.906861	26.296295
207.129194	6905.814199	26.301312
206.941319	6918.131706	26.306330
207.389421	6933.114300	26.311348
207.841797	6930.572110	26.316365
207.931510	6932.382214	26.321383
208.156119	6948.351722	26.326400
208.278582	6964.387103	26.331418
208.787418	6965.932899	26.336436
208.924397	6966.113827	26.341453
209.017292	6968.015487	26.346471
209.338036	6969.703786	26.351488
209.301476	6981.123847	26.356506
209.346605	6990.324635	26.361524
209.779449	6990.374991	26.366541
209.787484	7009.122754	26.371559
210.147575	7017.499895	26.376576
209.979536	7026.767735	26.381594
210.353516	7030.062912	26.386612
210.361379	7045.388048	26.391629
210.447422	7063.811858	26.396647
211.192267	7065.077697	26.401664
211.120054	7072.808561	26.406682
211.317849	7086.441675	26.411700
211.801245	7097.084159	26.416717
212.047286	7095.325474	26.421735
212.125207	7108.867562	26.426752
212.488134	7125.235379	26.431770
212.936473	7126.383259	26.436788
213.177802	7123.172042	26.441805
213.090635	7127.774512	26.446823
213.242436	7125.149594	26.451840
213.453668	7138.074038	26.456858
213.487371	7143.715534	26.461876
213.705093	7148.033354	26.466893
213.814659	7159.061230	26.471911
214.046102	7174.516091	26.476928
213.931374	7180.357515	26.481946
214.578578	7193.303776	26.486964
214.595869	7206.622716	26.491981
214.827707	7215.341445	26.496999
215.321778	7227.020161	26.502016
215.623027	7237.397509	26.507034
215.620165	7238.277416	26.512052
215.824696	7246.624409	26.517069
215.940456	7259.321045	26.522087
216.460758	7261.959542	26.527104
216.602084	7275.213132	26.532122
216.843410	7286.751216	26.537140
217.009952	7292.495912	26.542157
216.829390	7312.130600	26.547175
216.973402	7322.542516	26.552192
217.620091	7322.786183	26.557210
217.526656	7338.108885	26.562228
217.725751	7353.469946	26.567245
218.227293	7366.125629	26.572263
218.856532	7371.944520	26.577280
218.580355	7380.503561	26.582298
218.962176	7381.780094	26.587316
219.139399	7392.220600	26.592333
219.374333	7408.539892	26.597351
219.843554	7405.097146	26.602368
219.808679	7428.696112	26.607386
220.111123	7432.367096	26.612404
220.188818	7441.347374	26.617421
220.388530	7452.096715	26.622439
220.702211	7453.480114	26.627456
220.621013	7473.588987	26.632474
221.007362	7485.204036	26.637492
221.341152	7486.818714	26.642509
221.396426	7501.530885	26.647527
222.066295	7514.576893	26.652544
221.811627	7521.233908	26.657562
222.244292	7525.304336	26.662580
222.414131	7540.800086	26.667597
222.944489	7556.483877	26.672615
223.147957	7543.130535	26.677632
223.242967	7562.718867	26.682650
223.760757	7571.664473	26.687668
223.787732	7573.998475	26.692685
223.700359	7572.762642	26.697703
224.141840	7581.903756	26.702720
224.392596	7601.279251	26.707738
224.249029	7606.596671	26.712756
224.810137	7613.769688	26.717773
224.719621	7614.838273	26.722791
225.096308	7623.922074	26.727808
225.142818	7637.180087	26.732826
225.311588	7634.653094	26.737844
225.428718	7663.707104	26.742861
225.363154	7672.404270	26.747879
225.950693	7682.515183	26.752896
226.490575	7696.072290	26.757914
226.282581	7699.538296	26.762932
226.734832	7713.249450	26.767949
227.069553	7724.529058	26.772967
227.425857	7731.349218	26.777984
227.550342	7735.756040	26.783002
227.689836	7743.208000	26.788020
228.222394	7740.858268	26.793037
228.164772	7763.307058	26.798055
228.359268	7772.154820	26.803072
228.436532	7775.658777	26.808090
228.675229	7787.531301	26.813108
228.959265	7799.477654	26.818125
229.164441	7817.932980	26.823143
229.617285	7824.622910	26.828160
229.515002	7833.692706	26.833178
229.926363	7861.484481	26.838196
230.257063	7856.763806	26.843213
230.468120	7872.453983	26.848231
230.547659	7894.615142	26.853248
231.042244	7892.100690	26.858266
230.665020	7901.451206	26.863284
231.349957	7915.072733	26.868301
231.914809	7927.672380	26.873319
231.919981	7934.798837	26.878336
231.977430	7946.222748	26.883354
232.284513	7950.277906	26.888372
232.803295	7965.144052	26.893389
232.758396	7974.455012	26.898407
233.030697	7978.405559	26.903424
233.197841	7990.639026	26.908442
233.589712	8004.999809	26.913460
233.819066	8004.026625	26.918477
233.788772	8026.821616	26.923495
234.536416	8032.649438	26.928512
234.419959	8037.400069	26.933530
234.773783	8052.922892	26.938548
235.061713	8061.445900	26.943565
234.830560	8070.507268	26.948583
235.288596	8086.553314	26.953600
235.683031	8097.038377	26.958618
235.569401	8107.328244	26.963636
236.122730	8114.081763	26.968653
236.141386	8130.252982	26.973671
236.745080	8133.156119	26.978688
236.989815	8155.554151	26.983706
236.919911	8157.310375	26.988724
237.199757	8148.616069	26.993741
237.403259	8172.084963	26.998759
237.580101	8183.142612	27.003776
237.878470	8193.052891	27.008794
238.027709	8196.810655	27.013812
237.958469	8202.471323	27.018829
238.444297	8207.129144	27.023847
238.872069	8226.065690	27.028864
238.987553	8236.758600	27.033882
239.228058	8234.871225	27.038900
239.677063	8254.799841	27.043917
239.837213	8269.046736	27.048935
239.965128	8270.730520	27.053952
240.046012	8289.638249	27.058970
240.052417	8296.125723	27.063988
240.474706	8309.870536	27.069005
240.394904	8333.988788	27.074023
240.835719	8338.088047	27.079040
241.302303	8353.496420	27.084058
241.206293	8371.469682	27.089076
241.749457	8367.871721	27.094093
241.996919	8382.469532	27.099111
242.347813	8406.149401	27.104128
242.797644	8408.878824	27.109146
242.890941	8413.892798	27.114164
243.343447	8424.853960	27.119181
243.379631	8440.259426	27.124199
243.441554	8446.142037	27.129216
244.017965	8454.819552	27.134234
243.798412	8469.615440	27.139252
244.515351	8479.070456	27.144269
244.647904	8501.982247	27.149287
244.721861	8500.685600	27.154304
245.232611	8508.150370	27.159322
245.609343	8520.942615	27.164340
245.800321	8522.880383	27.169357
245.774659	8542.339332	27.174375
246.264795	8547.882632	27.179392
246.484255	8559.479094	27.184410
246.416417	8565.466243	27.189428
246.791418	8577.202782	27.194445
246.977460	8582.938182	27.199463
246.818199	8607.083706	27.204480
247.175288	8620.170325	27.209498
247.563235	8635.630085	27.214516
247.893501	8650.057183	27.219533
247.876538	8672.302160	27.224551
247.963681	8681.733762	27.229568
248.853625	8699.296467	27.234586
248.507429	8720.508448	27.239604
249.201349	8728.035413	27.244621
249.505188	8743.208483	27.249639
249.812150	8747.510580	27.254656
249.887791	8758.406945	27.259674
250.209325	8773.792842	27.264692
250.757827	8765.848176	27.269709
250.380420	8788.899930	27.274727
250.560145	8809.127570	27.279744
250.927370	8808.100490	27.284762
251.000133	8835.638798	27.289780
251.323710	8836.879897	27.294797
251.663978	8855.820178	27.299815
251.857375	8868.846154	27.304832
252.367071	8892.689163	27.309850
252.423303	8894.920342	27.314868
252.804056	8901.652946	27.319885
252.988769	8922.926557	27.324903
253.270572	8937.112596	27.329920
253.655946	8936.847903	27.334938
253.678121	8956.289926	27.339956
253.971999	8965.693081	27.344973
254.295941	8983.587149	27.349991
254.933305	8993.332967	27.355008
255.427684	9006.011657	27.360026
255.393713	9012.265077	27.365044
255.846090	9011.206312	27.370061
255.671318	9029.361714	27.375079
255.762879	9049.305485	27.380096
256.367510	9052.157511	27.385114
256.267867	9078.076694	27.390132
256.794393	9086.273453	27.395149
257.160929	9091.229541	27.400167
257.416150	9102.717243	27.405184
257.571534	9111.938357	27.410202
257.640693	9130.205695	27.415220
257.855864	9126.223486	27.420237
257.985031	9146.918427	27.425255
258.073331	9165.662790	27.430272
258.695360	9175.334840	27.435290
258.632753	9190.583698	27.440308
259.312435	9214.854584	27.445325
259.715369	9228.543918	27.450343
259.742231	9240.887729	27.455360
260.483238	9248.405489	27.460378
260.373650	9258.680941	27.465396
260.740084	9255.210102	27.470413
260.900339	9285.309387	27.475431
261.089835	9288.300034	27.480448
261.726749	9290.180592	27.485466
261.649087	9317.183064	27.490484
261.835310	9323.905947	27.495501
262.270283	9334.512516	27.500519
262.297799	9345.865541	27.505536
262.472203	9353.301724	27.510554
262.694984	9372.194497	27.515572
263.052843	9384.181114	27.520589
263.161166	9408.216020	27.525607
263.334943	9423.973973	27.530624
263.734653	9432.742794	27.535642
263.656240	9447.369984	27.540660
264.048915	9472.940659	27.545677
264.387436	9483.524935	27.550695
264.760151	9493.892863	27.555712
265.054549	9509.917739	27.560730
265.337923	9524.220949	27.565748
265.343859	9531.423198	27.570765
265.903430	9541.200273	27.575783
266.393083	9557.420720	27.580800
266.652309	9554.269096	27.585818
266.722492	9575.906973	27.590836
266.943936	9588.238547	27.595853
267.386037	9595.441341	27.600871
267.647779	9613.048213	27.605888
268.146170	9616.038479	27.610906
268.071768	9641.782659	27.615924
268.453595	9639.588886	27.620941
268.665788	9648.745008	27.625959
268.673373	9673.102131	27.630976
269.234913	9677.460323	27.635994
269.591615	9701.057508	27.641012
269.894634	9696.666482	27.646029
270.232672	9706.779994	27.651047
270.366165	9733.225827	27.656064
270.854863	9730.036410	27.661082
270.632311	9746.853000	27.666100
271.065520	9758.949495	27.671117
271.345630	9772.077728	27.676135
271.312364	9798.140244	27.681152
272.086099	9807.764918	27.686170
271.871920	9821.718821	27.691188
272.143061	9839.840323	27.696205
272.586105	9851.784226	27.701223
272.600538	9868.224778	27.706240
273.313329	9875.611604	27.711258
273.518741	9901.195940	27.716276
273.904601	9915.028314	27.721293
274.306070	9915.040030	27.726311
274.490053	9922.729165	27.731328
275.030785	9936.542382	27.736346
275.247264	9935.535720	27.741364
275.244742	9948.182668	27.746381
275.663828	9959.590215	27.751399
275.826857	9974.461171	27.756416
276.469729	9987.082009	27.761434
276.484410	9995.776387	27.766452
276.775245	10001.272127	27.771469
277.141878	10013.539199	27.776487
276.990178	10028.637447	27.781504
277.458856	10034.935515	27.786522
277.639586	10053.703243	27.791540
277.632325	10062.474347	27.796557
277.914002	10083.078588	27.801575
277.946932	10102.206373	27.806592
278.799257	10116.891655	27.811610
278.889545	10137.563466	27.816628
279.143756	10151.876253	27.821645
279.572607	10162.020063	27.826663
279.793112	10169.667301	27.831680
279.979432	10186.112282	27.836698
280.318345	10193.711540	27.841716
280.847858	10211.047811	27.846733
281.186531	10217.786934	27.851751
281.284365	10218.427853	27.856768
281.445538	10234.895783	27.861786
281.631143	10261.026916	27.866804
281.232715	10276.485047	27.871821
281.992899	10291.991469	27.876839
282.115397	10316.689008	27.881856
282.357657	10328.234808	27.886874
282.687969	10346.419894	27.891892
282.803542	10373.011762	27.896909
282.966252	10385.925113	27.901927
283.584455	10406.493865	27.906944
283.943819	10433.491246	27.911962
284.089542	10446.345575	27.916980
284.602952	10458.618736	27.921997
284.958745	10464.003950	27.927015
284.950495	10495.159561	27.932032
285.502342	10515.543075	27.937050
285.892571	10531.411320	27.942068
286.175750	10549.769044	27.947085
286.428581	10562.509991	27.952103
286.745752	10583.421312	27.957120
287.200488	10591.242547	27.962138
287.517577	10611.052886	27.967156
287.567909	10621.019269	27.972173
288.145616	10628.037252	27.977191
288.689725	10654.021811	27.982208
288.687946	10649.574029	27.987226
289.103929	10673.122368	27.992244
289.252611	10682.731550	27.997261
289.603597	10691.733180	28.002279
289.674143	10716.531737	28.007296
290.285852	10712.587829	28.012314
290.482523	10739.175288	28.017332
290.485482	10752.120711	28.022349
291.150323	10756.139296	28.027367
291.223560	10783.003468	28.032384
291.452912	10794.477311	28.037402
291.753904	10806.749986	28.042420
291.915777	10820.949056	28.047437
292.512042	10835.508226	28.052455
292.666611	10849.718326	28.057472
293.131297	10858.468187	28.062490
293.417818	10874.243927	28.067508
293.207523	10890.863078	28.072525
293.971062	10897.707937	28.077543
294.055938	10913.084172	28.082560
294.549071	10934.028142	28.087578
294.868411	10945.541668	28.092596
294.838527	10950.504507	28.097613
295.144383	10957.876855	28.102631
295.174889	10974.543897	28.107648
295.831915	10983.068777	28.112666
296.043662	10992.971113	28.117684
295.782977	11020.814880	28.122701
296.621029	11031.506374	28.127719
296.913308	11054.542203	28.132736
297.156104	11071.463965	28.137754
297.204300	11078.528389	28.142772
297.742636	11087.519285	28.147789
298.160444	11093.605541	28.152807
298.134712	11119.306313	28.157824
298.690331	11138.975832	28.162842
299.220193	11153.443186	28.167860
299.203006	11171.112083	28.172877
299.686898	11174.141976	28.177895
300.035236	11194.573016	28.182912
300.438127	11209.755624	28.187930
300.645497	11212.785917	28.192948
301.060877	11232.394485	28.197965
301.546328	11244.130865	28.202983
301.329255	11261.171786	28.208000
301.714731	11269.571684	28.213018
302.102360	11286.999501	28.218036
302.241509	11303.704290	28.223053
302.517213	11303.955650	28.228071
302.561232	11330.869529	28.233088
302.904828	11342.524311	28.238106
303.145581	11369.931081	28.243124
303.365292	11381.299868	28.248141
304.108745	11400.241280	28.253159
304.120843	11431.287751	28.258176
304.654609	11441.103640	28.263194
305.210255	11457.089940	28.268212
305.240096	11480.913201	28.273229
305.524069	11482.162027	28.278247
305.868318	11516.186115	28.283264
306.439351	11522.382713	28.288282
306.858463	11532.680516	28.293300
306.923151	11549.168015	28.298317
307.448902	11569.917989	28.303335
307.560329	11583.171107	28.308352
307.674486	11593.516770	28.313370
308.258514	11609.528421	28.318388
308.083488	11625.510345	28.323405
309.139053	11642.210922	28.328423
309.187341	11656.518019	28.333440
309.315176	11673.174253	28.338458
309.603666	11692.168673	28.343476
309.683093	11712.131875	28.348493
310.232685	11718.893549	28.353511
310.107289	11749.375626	28.358528
310.565292	11765.890597	28.363546
310.919606	11783.457117	28.368564
310.902432	11808.477659	28.373581
311.906949	11816.544848	28.378599
312.399370	11830.071967	28.383616
312.256912	11840.938030	28.388634
312.544694	11858.557941	28.393652
312.624901	11866.283501	28.398669
312.942168	11879.780337	28.403687
313.040361	11911.864431	28.408704
313.487156	11930.631443	28.413722
314.238436	11948.863137	28.418740
314.342832	11966.634794	28.423757
314.640982	11977.154266	28.428775
314.782519	12005.008733	28.433792
315.290797	12017.875094	28.438810
315.686600	12031.584066	28.443828
316.261459	12056.628919	28.448845
316.750599	12061.636907	28.453863
316.767264	12083.309734	28.458880
316.993763	12090.575650	28.463898
317.656631	12106.395807	28.468916
317.845425	12116.724029	28.473933
318.071918	12130.145828	28.478951
318.694152	12146.098242	28.483968
318.522874	12156.381557	28.488986
318.887592	12177.881179	28.494004
318.923882	12195.627359	28.499021
319.527858	12210.984754	28.504039
319.501960	12243.079487	28.509056
319.876950	12257.621389	28.514074
320.683831	12269.086561	28.519092
320.939813	12291.906131	28.524109
321.134645	12305.381539	28.529127
321.463480	12325.961652	28.534144
321.689579	12337.533018	28.539162
322.102130	12372.594995	28.544180
322.017612	12384.136995	28.549197
322.733074	12392.813548	28.554215
322.778898	12421.922352	28.559232
323.280286	12441.591198	28.564250
323.761627	12458.455439	28.569268
323.896565	12479.121959	28.574285
324.636113	12496.790254	28.579303
325.078807	12518.145893	28.584320
325.250598	12530.905356	28.589338
325.478422	12542.330397	28.594356
325.440737	12575.079048	28.599373
325.853368	12584.231184	28.604391
326.014158	12605.056688	28.609408
326.304231	12621.712312	28.614426
326.997411	12644.522358	28.619444
327.289776	12678.599634	28.624461
327.418844	12690.961657	28.629479
327.501535	12705.998646	28.634496
327.878330	12727.674816	28.639514
328.881615	12742.726679	28.644532
328.919380	12766.845867	28.649549
329.252717	12767.118378	28.654567
329.572395	12788.087059	28.659584
329.414461	12796.565562	28.664602
330.110565	12816.200320	28.669620
330.104105	12844.650977	28.674637
330.768783	12850.459515	28.679655
330.630182	12876.345168	28.684672
331.285222	12897.988257	28.689690
331.422829	12914.623045	28.694708
331.554755	12948.470283	28.699725
332.635573	12960.387239	28.704743
332.693527	12979.729558	28.709760
332.928894	12994.495732	28.714778
333.333229	13017.483631	28.719796
333.659916	13029.077670	28.724813
334.474634	13046.007114	28.729831
334.636717	13068.577157	28.734848
334.804129	13078.159295	28.739866
335.474258	13102.782760	28.744884
335.465810	13121.956964	28.749901
335.757166	13136.702152	28.754919
336.307455	13148.723686	28.759936
336.581042	13175.646261	28.764954
337.021093	13178.949418	28.769972
336.969514	13198.334659	28.774989
337.569008	13226.760301	28.780007
338.145030	13230.531998	28.785024
338.057748	13247.476526	28.790042
338.603996	13260.720257	28.795060
338.584833	13297.358308	28.800077
339.075098	13314.310440	28.805095
339.376840	13329.309986	28.810112
339.450890	13352.537389	28.815130
340.151529	13367.843267	28.820148
340.208664	13394.577270	28.825165
340.538212	13421.528259	28.830183
341.177542	13449.846819	28.835200
341.496527	13463.309176	28.840218
341.962947	13484.453034	28.845236
341.985878	13511.392141	28.850253
342.589588	13523.633935	28.855271
342.984905	13540.668460	28.860288
343.274914	13567.312323	28.865306
343.795288	13589.066320	28.870324
344.146764	13603.702902	28.875341
344.609858	13626.213007	28.880359
344.795532	13630.269491	28.885376
345.100939	13653.257391	28.890394
345.643306	13658.906853	28.895412
345.579882	13683.945424	28.900429
346.154768	13711.616271	28.905447
346.431346	13719.290225	28.910464
346.881935	13746.010846	28.915482
347.032453	13761.548356	28.920500
347.272578	13777.751921	28.925517
347.707951	13793.116051	28.930535
347.967757	13813.916703	28.935552
348.277457	13829.182919	28.940570
348.697245	13843.582825	28.945588
348.865680	13871.309389	28.950605
349.077837	13877.041373	28.955623
349.796981	13890.202705	28.960640
350.180084	13915.943708	28.965658
350.529083	13930.673494	28.970676
350.546487	13950.011894	28.975693
350.932636	13977.287434	28.980711
351.313794	13993.690051	28.985728
351.393938	14017.531307	28.990746
351.817330	14033.861900	28.995764
352.166973	14064.830134	29.000781
352.425729	14087.236613	29.005799
353.097914	14108.888835	29.010816
353.216929	14140.211215	29.015834
353.675824	14158.073584	29.020852
354.108743	14183.335369	29.025869
354.504732	14208.012287	29.030887
354.977280	14223.631885	29.035904
355.116409	14257.669807	29.040922
355.821821	14273.251559	29.045940
355.807406	14305.155122	29.050957
355.989968	14322.557416	29.055975
356.610023	14349.469358	29.060992
357.243062	14372.695036	29.066010
357.308111	14396.058301	29.071028
357.636340	14409.098863	29.076045
358.176711	14430.146814	29.081063
358.765317	14449.411053	29.086080
359.098712	14476.756212	29.091098
359.449569	14482.561870	29.096116
359.403739	14514.124818	29.101133
360.089687	14534.648354	29.106151
360.635469	14552.430524	29.111168
360.698970	14580.601770	29.116186
361.110438	14591.691184	29.121204
361.895733	14616.590712	29.126221
362.019990	14639.985554	29.131239
362.415499	14650.676956	29.136256
362.662028	14674.431512	29.141274
362.996781	14684.984523	29.146292
363.275382	14708.090070	29.151309
363.444032	14737.982161	29.156327
363.996629	14752.837546	29.161344
364.032915	14782.908657	29.166362
364.182236	14800.293175	29.171380
364.867221	14835.838457	29.176397
365.335294	14855.838604	29.181415
365.846074	14877.518429	29.186432
366.108315	14908.210727	29.191450
366.617946	14919.341811	29.196468
366.944638	14934.747932	29.201485
367.347078	14954.631037	29.206503
367.857827	14972.679857	29.211520
367.957144	14982.240980	29.216538
368.287680	15000.434670	29.221556
368.392432	15016.513809	29.226573
369.100242	15042.096423	29.231591
369.290512	15061.372070	29.236608
369.370965	15084.765223	29.241626
370.079453	15099.495730	29.246644
370.520857	15121.824529	29.251661
370.389522	15150.166227	29.256679
370.951800	15172.527207	29.261696
371.592989	15199.496521	29.266714
371.954611	15208.714172	29.271732
372.627725	15237.722176	29.276749
372.674528	15248.177593	29.281767
373.291444	15277.514254	29.286784
373.248025	15307.877881	29.291802
373.881653	15324.191214	29.296820
374.103820	15340.636657	29.301837
374.398660	15367.452443	29.306855
375.075865	15389.052939	29.311872
375.132750	15408.821553	29.316890
375.397023	15436.466497	29.321908
375.827475	15464.353270	29.326925
376.025417	15483.084912	29.331943
376.471387	15499.758104	29.336960
376.647328	15533.384692	29.341978
377.027127	15563.030604	29.346996
377.502151	15593.469535	29.352013
377.911650	15621.150714	29.357031
378.706524	15642.761454	29.362048
379.209200	15674.343396	29.367066
379.406209	15699.414114	29.372084
379.838464	15724.590867	29.377101
380.084402	15749.296248	29.382119
380.589409	15776.125017	29.387136
380.572056	15800.188877	29.392154
381.098893	15828.369961	29.397172
381.510647	15851.422355	29.402189
381.741935	15879.887996	29.407207
382.371031	15906.821808	29.412224
382.582235	15938.671377	29.417242
383.079055	15970.543796	29.422260
383.357090	15994.577225	29.427277
383.677717	16013.093041	29.432295
384.815072	16037.151196	29.437312
384.837921	16059.316987	29.442330
385.413363	16070.439312	29.447348
386.213950	16092.072019	29.452365
386.205136	16113.032856	29.457383
386.600023	16138.306191	29.462400
387.158911	16143.784689	29.467418
387.486444	16166.604748	29.472436
387.962606	16178.168313	29.477453
388.018564	16194.433307	29.482471
388.486560	16203.616402	29.487488
388.510792	16229.837227	29.492506
388.817710	16245.783579	29.497524
389.503012	16265.070425	29.502541
389.551144	16296.884326	29.507559
390.022942	16306.462894	29.512576
390.645623	16344.409610	29.517594
390.805621	16365.340346	29.522612
391.100894	16389.102384	29.527629
391.355292	16420.697866	29.532647
392.045286	16439.045704	29.537664
392.004011	16472.303782	29.542682
392.237477	16495.041494	29.547700
393.145505	16516.253392	29.552717
393.148117	16537.116733	29.557735
393.752933	16576.335438	29.562752
393.818575	16592.686308	29.567770
394.670741	16632.157838	29.572788
394.970262	16651.957782	29.577805
395.007642	16693.918135	29.582823
395.734394	16716.852938	29.587840
395.985911	16747.910030	29.592858
396.548831	16775.620803	29.597876
397.045836	16795.002685	29.602893
397.567992	16829.153358	29.607911
398.102498	16854.431800	29.612928
398.169060	16875.542275	29.617946
398.522860	16904.106615	29.622964
399.337205	16929.613205	29.627981
399.387517	16960.590787	29.632999
400.201377	16985.610969	29.638016
400.456766	17014.503770	29.643034
401.034700	17036.713015	29.648052
401.287869	17054.217872	29.653069
401.507285	17088.433697	29.658087
402.243709	17106.607820	29.663104
402.562990	17134.614934	29.668122
402.596099	17156.000397	29.673140
403.208710	17179.789066	29.678157
403.437466	17210.926105	29.683175
403.922242	17231.663554	29.688192
404.201203	17261.744330	29.693210
404.737657	17291.492025	29.698228
405.746457	17313.866860	29.703245
405.696126	17347.318210	29.708263
406.402015	17353.997678	29.713280
406.750746	17385.359246	29.718298
407.226410	17400.247080	29.723316
407.347130	17424.157613	29.728333
407.599623	17452.544236	29.733351
408.389982	17472.672319	29.738368
408.911898	17491.272794	29.743386
408.895068	17512.084248	29.748404
409.765513	17524.017679	29.753421
409.926203	17547.628345	29.758439
409.966444	17560.670432	29.763456
410.397533	17575.478533	29.768474
410.633567	17599.298918	29.773492
411.144140	17617.885212	29.778509
411.499175	17647.092833	29.783527
412.067314	17660.855982	29.788544
412.542968	17694.234505	29.793562
412.635718	17724.871034	29.798580
413.029895	17741.509932	29.803597
413.193312	17781.902005	29.808615
413.485868	17807.404217	29.813632
414.028449	17837.768903	29.818650
414.391162	17868.885132	29.823668
414.918890	17899.623954	29.828685
415.235076	17938.521247	29.833703
415.836274	17966.168216	29.838720
416.392994	17997.261664	29.843738
416.620066	18026.070312	29.848756
417.395429	18054.248346	29.853773
417.701142	18086.887867	29.858791
418.093159	18110.514499	29.863808
418.633413	18137.055738	29.868826
419.095667	18171.100809	29.873844
419.467673	18197.997307	29.878861
419.914951	18237.519346	29.883879
420.267843	18255.256328	29.888896
420.753234	18283.770750	29.893914
421.189059	18308.677724	29.898932
421.690910	18339.313272	29.903949
421.929005	18366.192816	29.908967
422.472092	18392.158441	29.913984
422.830046	18423.144647	29.919002
423.511188	18451.475428	29.924020
424.025251	18463.622679	29.929037
424.100215	18502.774391	29.934055
424.710062	18519.842766	29.939072
425.306795	18549.405711	29.944090
425.180751	18581.957186	29.949108
425.869424	18598.897731	29.954125
426.323467	18635.585367	29.959143
426.459923	18650.444593	29.964160
426.986122	18695.878258	29.969178
427.347029	18724.868853	29.974196
427.944373	18747.376689	29.979213
428.102982	18788.937936	29.984231
428.754904	18805.009722	29.989248
429.510049	18831.958088	29.994266
429.605211	18865.111158	29.999284
430.481381	18890.723745	30.004301
430.510267	18917.294644	30.009319
431.200335	18942.005031	30.014336
431.605064	18966.114429	30.019354
431.790785	18986.284130	30.024372
432.492141	19002.512034	30.029389
432.569922	19038.635732	30.034407
432.980255	19059.181969	30.039424
433.631214	19084.131898	30.044442
433.533828	19116.301157	30.049460
433.972601	19141.729897	30.054477
434.378235	19170.632694	30.059495
434.782870	19201.052344	30.064512
435.311902	19231.177804	30.069530
435.920505	19261.282375	30.074548
436.621072	19282.431531	30.079565
436.950701	19317.037289	30.084583
437.085254	19347.097469	30.089600
437.576875	19373.652115	30.094618
437.828062	19405.345137	30.099636
438.558865	19434.816745	30.104653
438.766729	19468.193709	30.109671
439.356409	19502.395816	30.114688
439.646921	19538.471025	30.119706
440.380555	19552.599686	30.124724
441.184468	19577.105526	30.129741
441.275525	19616.494890	30.134759
441.574385	19648.539111	30.139776
442.043032	19669.339093	30.144794
442.445405	19708.142812	30.149812
443.087706	19727.835961	30.154829
443.165569	19769.997388	30.159847
444.112706	19803.854197	30.164864
444.567860	19832.810967	30.169882
444.637495	19856.691637	30.174900
445.540512	19882.378365	30.179917
445.832492	19906.411501	30.184935
446.070426	19942.220004	30.189952
446.609296	19964.894056	30.194970
447.245545	20003.629747	30.199988
447.833165	20037.323845	30.205005
447.994804	20066.956631	30.210023
448.317187	20094.137966	30.215040
448.884488	20125.414714	30.220058
449.117659	20162.298237	30.225076
449.663526	20191.611741	30.230093
450.205999	20223.611633	30.235111
450.616431	20247.787073	30.240128
451.444336	20277.864181	30.245146
451.546748	20308.674344	30.250164
451.996954	20347.632287	30.255181
452.405771	20376.723056	30.260199
452.983636	20401.863147	30.265216
453.902954	20432.465831	30.270234
454.015513	20465.127713	30.275252
454.854734	20489.164728	30.280269
454.841782	20515.171295	30.285287
455.238870	20549.746982	30.290304
455.819803	20569.027285	30.295322
455.802320	20599.438551	30.300340
456.227905	20632.667149	30.305357
456.919242	20654.439818	30.310375
457.598276	20680.097789	30.315392
458.111273	20706.373691	30.320410
458.319111	20736.152374	30.325428
458.823723	20759.143325	30.330445
458.984866	20794.473012	30.335463
459.445452	20818.974472	30.340480
459.866184	20848.504452	30.345498
460.373526	20879.672161	30.350516
460.833868	20913.162792	30.355533
461.380702	20948.470753	30.360551
461.800437	20969.679938	30.365568
462.437718	21003.279604	30.370586
462.599532	21041.290546	30.375604
463.083050	21061.823427	30.380621
463.340791	21105.812492	30.385639
463.717992	21147.186871	30.390656
464.304022	21180.950232	30.395674
464.914310	21223.480823	30.400692
465.616418	21253.611746	30.405709
465.864433	21292.662527	30.410727
466.083768	21319.805306	30.415744
466.891943	21357.787278	30.420762
467.377706	21400.778436	30.425780
468.024512	21429.833243	30.430797
468.735263	21467.810526	30.435815
468.719019	21502.495902	30.440832
469.340572	21526.762541	30.445850
469.908891	21557.873052	30.450868
470.508843	21598.882350	30.455885
470.867196	21633.171252	30.460903
471.291555	21658.494937	30.465920
471.609496	21690.040963	30.470938
472.025091	21729.878124	30.475956
472.830001	21765.483104	30.480973
473.171411	21795.924560	30.485991
473.610058	21826.679795	30.491008
474.082600	21862.677396	30.496026
474.559409	21894.673438	30.501044
474.934290	21932.235159	30.506061
475.644274	21966.514447	30.511079
476.219077	22000.148252	30.516096
476.862270	22027.362552	30.521114
477.075718	22070.839189	30.526132
477.651078	22092.565390	30.531149
478.022474	22121.889031	30.536167
478.163127	22163.699140	30.541184
478.834782	22190.869808	30.546202
479.055284	22231.044907	30.551220
479.642155	22267.335535	30.556237
480.010169	22303.022361	30.561255
480.657561	22337.440020	30.566272
481.307306	22371.988912	30.571290
481.604725	22417.443426	30.576308
482.404912	22435.690036	30.581325
482.870998	22455.682485	30.586343
483.025802	22487.135588	30.591360
483.392524	22510.029776	30.596378
483.879616	22557.262067	30.601396
484.525230	22594.404174	30.606413
484.488977	22628.646259	30.611431
484.773829	22667.314147	30.616448
485.618005	22692.770308	30.621466
485.680323	22742.543981	30.626484
486.292667	22784.583036	30.631501
487.216605	22820.862195	30.636519
487.283109	22864.295896	30.641536
488.074554	22898.303524	30.646554
488.539912	22932.966507	30.651572
489.323677	22970.009512	30.656589
489.720925	23010.668038	30.661607
490.326192	23038.851055	30.666624
491.054743	23070.972419	30.671642
491.387106	23107.816707	30.676660
491.836320	23138.657880	30.681677
492.609211	23171.289084	30.686695
493.094638	23190.337349	30.691712
493.999478	23228.555757	30.696730
494.566914	23263.637203	30.701748
495.061859	23279.350687	30.706765
495.349485	23310.162800	30.711783
495.600958	23337.916725	30.716800
496.339423	23355.063632	30.721818
496.525998	23401.164818	30.726836
497.062242	23428.148884	30.731853
497.350558	23459.153367	30.736871
497.981929	23494.603220	30.741888
498.252746	23532.435009	30.746906
498.578216	23567.447762	30.751924
499.228573	23604.904193	30.756941
500.155217	23637.229091	30.761959
500.424964	23684.072442	30.766976
501.183719	23707.438383	30.771994
501.559890	23745.633559	30.777012
501.866266	23788.670028	30.782029
502.583514	23815.869314	30.787047
502.935745	23854.654604	30.792064
503.196957	23888.599168	30.797082
503.685593	23926.228630	30.802100
504.149616	23965.465846	30.807117
504.705440	23997.290501	30.812135
505.217027	24046.920282	30.817152
506.097050	24079.802536	30.822170
506.606652	24117.680387	30.827188
506.670943	24152.182280	30.832205
507.625046	24186.058061	30.837223
507.837081	24220.688593	30.842240
508.674237	24245.938849	30.847258
509.075571	24285.424728	30.852276
509.455742	24312.674624	30.857293
509.788685	24345.026224	30.862311
510.204072	24373.071717	30.867328
510.786682	24404.966967	30.872346
511.031541	24434.177193	30.877364
511.221527	24481.301842	30.882381
511.728838	24518.991961	30.887399
512.221418	24564.235626	30.892416
512.685370	24609.784104	30.897434
513.193011	24654.367087	30.902452
513.794291	24694.917859	30.907469
514.535291	24731.769346	30.912487
514.871398	24785.193947	30.917504
515.477183	24815.239091	30.922522
516.246517	24864.559379	30.927540
516.637290	24910.241683	30.932557
517.359219	24947.707206	30.937575
517.757129	24988.733831	30.942592
518.353910	25023.827091	30.947610
518.677191	25070.855834	30.952628
519.223984	25101.694724	30.957645
519.894283	25141.101276	30.962663
520.112875	25190.446493	30.967680
521.059425	25228.538608	30.972698
521.459071	25280.491880	30.977716
522.134545	25318.231937	30.982733
522.845511	25352.663343	30.987751
523.596453	25392.995107	30.992768
524.261163	25418.751295	30.997786
524.910867	25457.403291	31.002804
525.143070	25486.140857	31.007821
525.884194	25516.752652	31.012839
525.850194	25557.423352	31.017856
526.514979	25583.083685	31.022874
527.121893	25616.427777	31.027892
527.070451	25658.907880	31.032909
528.155026	25688.582199	31.037927
528.517025	25736.069941	31.042944
529.073162	25778.665492	31.047962
529.498379	25825.150035	31.052980
529.561860	25863.365424	31.057997
530.280321	25902.507000	31.063015
530.595814	25951.538976	31.068032
531.552664	25981.529606	31.073050
532.260596	26028.026424	31.078068
532.840713	26081.088757	31.083085
533.512766	26121.643692	31.088103
533.816576	26157.618024	31.093120
534.387903	26190.775970	31.098138
534.728265	26230.455194	31.103156
534.984574	26271.935439	31.108173
535.948924	26320.156947	31.113191
536.384620	26370.496938	31.118208
536.854448	26402.358995	31.123226
537.574112	26429.895607	31.128244
537.912252	26466.801087	31.133261
538.720474	26505.420909	31.138279
539.186735	26542.701639	31.143296
539.700475	26567.134189	31.148314
540.105746	26611.891767	31.153332
540.580506	26652.306936	31.158349
541.288890	26684.655458	31.163367
541.695086	26726.790533	31.168384
542.302601	26759.336473	31.173402
542.739525	26788.154844	31.178420
542.926203	26829.297032	31.183437
543.436045	26871.968248	31.188455
543.793336	26925.430478	31.193472
544.397265	26969.582284	31.198490
544.900448	27022.352720	31.203508
545.181466	27078.132047	31.208525
546.031534	27113.742609	31.213543
546.447116	27171.223847	31.218560
547.031375	27229.195255	31.223578
547.768925	27272.806625	31.228596
548.224571	27323.761733	31.233613
548.956166	27362.866172	31.238631
549.740561	27418.000023	31.243648
550.115651	27464.220745	31.248666
550.716990	27512.343715	31.253684
551.353055	27563.255084	31.258701
551.967297	27600.454813	31.263719
552.790401	27648.675230	31.268736
553.225839	27692.113675	31.273754
554.152708	27727.166576	31.278772
554.291446	27769.568368	31.283789
554.956631	27813.320364	31.288807
555.542283	27856.932297	31.293824
556.054831	27889.429466	31.298842
556.498882	27938.303613	31.303860
557.050559	27979.233014	31.308877
558.033156	28014.841794	31.313895
558.254779	28064.632614	31.318912
558.809191	28105.125404	31.323930
559.503149	28143.484502	31.328948
560.210816	28193.089571	31.333965
560.621699	28231.913129	31.338983
560.971182	28276.354864	31.344000
561.678877	28318.544557	31.349018
562.384977	28358.230642	31.354036
562.575961	28405.209827	31.359053
563.383636	28447.365022	31.364071
563.778922	28495.063596	31.369088
564.415487	28539.164069	31.374106
565.202292	28585.872384	31.379124
565.487888	28628.635960	31.384141
566.092498	28666.993196	31.389159
566.830691	28713.498458	31.394176
567.534936	28748.652072	31.399194
568.044879	28782.709970	31.404212
568.405036	28824.557644	31.409229
568.965545	28857.112152	31.414247
569.484841	28893.014131	31.419264
569.929287	28930.283361	31.424282
570.856473	28971.199585	31.429300
571.327643	29008.617599	31.434317
571.783266	29041.275856	31.439335
572.161612	29078.975140	31.444352
572.951976	29116.670348	31.449370
573.396713	29151.056160	31.454388
573.624191	29201.872289	31.459405
574.289273	29236.089234	31.464423
575.088829	29274.654820	31.469440
575.128119	29320.020291	31.474458
576.148129	29370.575191	31.479476
576.333312	29426.380224	31.484493
577.174760	29470.447444	31.489511
577.439703	29521.153015	31.494528
578.222224	29567.089480	31.499546
579.150606	29609.981770	31.504564
579.542847	29659.911047	31.509581
580.659603	29701.848499	31.514599
581.121342	29741.299521	31.519616
581.344391	29782.843699	31.524634
582.277974	29835.130024	31.529652
582.487226	29876.648270	31.534669
583.328431	29921.146990	31.539687
583.804305	29972.446028	31.544704
584.639169	30017.946765	31.549722
585.289157	30041.873530	31.554740
585.858132	30094.965774	31.559757
586.421461	30128.293036	31.564775
587.462605	30172.828368	31.569792
587.854788	30214.264755	31.574810
588.602285	30253.028497	31.579828
588.927053	30287.016598	31.584845
589.457689	30330.494218	31.589863
589.923751	30364.677466	31.594880
590.451824	30414.507042	31.599898
591.505107	30445.626148	31.604916
591.402953	30504.583808	31.609933
592.006400	30547.358533	31.614951
592.628119	30594.472430	31.619968
593.016863	30638.684258	31.624986
593.395892	30698.847299	31.630004
594.083827	30740.471171	31.635021
594.742016	30790.224430	31.640039
595.426954	30841.324261	31.645056
595.446543	30893.157490	31.650074
596.789262	30945.158413	31.655092
597.260337	31003.809074	31.660109
598.029495	31055.405232	31.665127
598.771075	31095.837831	31.670144
599.148844	31139.466456	31.675162
599.702257	31187.910547	31.680180
600.058459	31239.590389	31.685197
600.910037	31274.711810	31.690215
601.681789	31322.412282	31.695232
602.167117	31365.653994	31.700250
602.832106	31392.855505	31.705268
603.057836	31446.411858	31.710285
603.660839	31491.179753	31.715303
604.172895	31530.883986	31.720320
604.634890	31577.472928	31.725338
605.378093	31625.360083	31.730356
605.861557	31682.532785	31.735373
606.628902	31729.568437	31.740391
607.138156	31782.160263	31.745408
607.730602	31839.257836	31.750426
608.558063	31886.367899	31.755444
608.694268	31945.032695	31.760461
609.231910	31994.038061	31.765479
610.180622	32053.281544	31.770496
610.609933	32103.855443	31.775514
611.225467	32155.558334	31.780532
612.008058	32216.494886	31.785549
612.709366	32263.878312	31.790567
613.688225	32318.130876	31.795584
614.128405	32370.732430	31.800602
614.863797	32420.686395	31.805620
615.421319	32472.867655	31.810637
616.093222	32514.334654	31.815655
616.746667	32568.992941	31.820672
617.175900	32619.721328	31.825690
618.042078	32676.009010	31.830708
618.355298	32726.384210	31.835725
619.396005	32765.827543	31.840743
619.822862	32821.402293	31.845760
620.290202	32872.301927	31.850778
620.916611	32914.992469	31.855796
621.471113	32977.951087	31.860813
621.988306	33024.768618	31.865831
622.826410	33079.301459	31.870848
623.478190	33145.159747	31.875866
624.425977	33196.117850	31.880884
624.953164	33249.983560	31.885901
625.701784	33297.239470	31.890919
626.328408	33331.023434	31.895936
626.758448	33387.972533	31.900954
627.762323	33429.127300	31.905972
627.835375	33486.206096	31.910989
628.764194	33541.317131	31.916007
629.798461	33582.026071	31.921024
629.751612	33633.533268	31.926042
630.573543	33679.391432	31.931060
630.946784	33737.425831	31.936077
632.084858	33778.556946	31.941095
632.606042	33821.859289	31.946112
632.743552	33881.061966	31.951130
633.518366	33925.657780	31.956148
634.270834	33964.699046	31.961165
634.519832	34022.519350	31.966183
635.373288	34056.383748	31.971200
635.904242	34099.688414	31.976218
636.942284	34154.478281	31.981236
637.209038	34206.347169	31.986253
638.050101	34252.858071	31.991271
638.492148	34292.911135	31.996288
638.803283	34352.688445	32.001306
639.496064	34397.210313	32.006324
640.569224	34456.737385	32.011341
640.944679	34511.465269	32.016359
641.432999	34559.038948	32.021376
641.662599	34610.547707	32.026394
642.240873	34669.665660	32.031412
642.776129	34729.903630	32.036429
643.590513	34795.952240	32.041447
644.534645	34846.521894	32.046464
645.053730	34916.494467	32.051482
646.228696	34964.756067	32.056500
646.893274	35021.271419	32.061517
647.400118	35077.774245	32.066535
648.369585	35125.730097	32.071552
648.878210	35185.704380	32.076570
649.546656	35230.221317	32.081588
650.581420	35285.223530	32.086605
651.069066	35333.876263	32.091623
652.045782	35381.979889	32.096640
652.501184	35435.142080	32.101658
653.292556	35486.873081	32.106676
653.609468	35533.031185	32.111693
654.249401	35585.057763	32.116711
655.042053	35629.937503	32.121728
655.749240	35690.965046	32.126746
656.420851	35739.368953	32.131764
656.871539	35792.306011	32.136781
657.506267	35836.229277	32.141799
658.451913	35888.361043	32.146816
659.295256	35943.957157	32.151834
659.711641	35986.047384	32.156852
660.340055	36039.559164	32.161869
660.968014	36092.532006	32.166887
661.482557	36144.853036	32.171904
662.138363	36197.536418	32.176922
662.880136	36253.045680	32.181940
663.411752	36307.850752	32.186957
663.822574	36367.015565	32.191975
664.914813	36416.439141	32.196992
665.295072	36472.632600	32.202010
665.949551	36524.893119	32.207028
666.855100	36576.267188	32.212045
666.842928	36634.374604	32.217063
668.025110	36694.193434	32.222080
668.669247	36749.823944	32.227098
669.168910	36793.935197	32.232116
669.982338	36849.376688	32.237133
670.554026	36906.357807	32.242151
671.414992	36947.701704	32.247168
671.915306	36999.469536	32.252186
672.501253	37050.878606	32.257204
673.298938	37105.561930	32.262221
673.898035	37151.845104	32.267239
674.566508	37200.225351	32.272256
675.358612	37254.758690	32.277274
676.008266	37308.250636	32.282292
676.387436	37371.077164	32.287309
676.749407	37422.997614	32.292327
677.815039	37479.633989	32.297344
678.197882	37539.370256	32.302362
679.027797	37598.264544	32.307380
679.770788	37649.618903	32.312397
680.505801	37710.603634	32.317415
680.980246	37769.583502	32.322432
681.260348	37835.891570	32.327450
682.910198	37893.465913	32.332468
683.356451	37950.811110	32.337485
683.831440	38010.215872	32.342503
684.970391	38068.001452	32.347520
685.343143	38130.738800	32.352538
686.183357	38187.659422	32.357556
687.016748	38236.440531	32.362573
687.652336	38292.853261	32.367591
688.268706	38346.347492	32.372608
689.132075	38410.116225	32.377626
690.232261	38461.390953	32.382644
690.551144	38512.109069	32.387661
690.882594	38575.832247	32.392679
691.752784	38621.899690	32.397696
692.462788	38697.470984	32.402714
693.268399	38745.270909	32.407732
693.966352	38803.372051	32.412749
694.691286	38862.503487	32.417767
695.252946	38918.835465	32.422784
695.907533	38983.502120	32.427802
696.477050	39036.564481	32.432820
697.200699	39093.968723	32.437837
697.702943	39166.391555	32.442855
698.927064	39223.505254	32.447872
699.500867	39287.350200	32.452890
699.916610	39345.414558	32.457908
700.937654	39399.656612	32.462925
701.624611	39464.625857	32.467943
702.554498	39520.193188	32.472960
703.292488	39573.178365	32.477978
704.272945	39623.632048	32.482996
704.870173	39666.815944	32.488013
705.380453	39729.578304	32.493031
706.289268	39781.371608	32.498048
706.574285	39837.864217	32.503066
707.231314	39880.435179	32.508084
707.840926	39933.224304	32.513101
708.539472	39990.555150	32.518119
709.310093	40039.759867	32.523136
709.896139	40097.457484	32.528154
710.536574	40150.406375	32.533172
711.553231	40192.321626	32.538189
711.880117	40252.574667	32.543207
712.479227	40300.973243	32.548224
713.285106	40363.358139	32.553242
713.660562	40422.137479	32.558260
714.336426	40475.056507	32.563277
715.147408	40551.914649	32.568295
716.152971	40613.161633	32.573312
716.555870	40688.309687	32.578330
717.298304	40747.015947	32.583348
717.848779	40803.813269	32.588365
718.415037	40881.077716	32.593383
719.378629	40940.008057	32.598400
720.147733	41010.106420	32.603418
720.595319	41079.821002	32.608436
721.673596	41144.373207	32.613453
722.072772	41214.714238	32.618471
723.108765	41278.018363	32.623488
723.811361	41342.905533	32.628506
724.828376	41417.110561	32.633524
725.699359	41471.584965	32.638541
726.461238	41542.828447	32.643559
727.428208	41608.447291	32.648576
727.937789	41663.787303	32.653594
728.309747	41729.170154	32.658612
729.303016	41786.401749	32.663629
729.990083	41858.229353	32.668647
730.805972	41916.716598	32.673664
731.306565	41981.382853	32.678682
732.042619	42051.124846	32.683700
733.268874	42112.297901	32.688717
733.707638	42179.428731	32.693735
734.620385	42236.059568	32.698752
735.663174	42300.322123	32.703770
736.142721	42361.769504	32.708788
736.710066	42420.260181	32.713805
737.199053	42499.465168	32.718823
738.272894	42549.384283	32.723840
738.924235	42615.624999	32.728858
740.029226	42683.711581	32.733876
740.900735	42738.167840	32.738893
740.957354	42804.882484	32.743911
741.717477	42862.287262	32.748928
742.337906	42934.707214	32.753946
743.185243	43006.085095	32.758964
744.049474	43069.136117	32.763981
744.769082	43144.187700	32.768999
745.457729	43200.810071	32.774016
745.990434	43276.097019	32.779034
746.833084	43331.805750	32.784052
748.038022	43385.425513	32.789069
748.450398	43444.537369	32.794087
749.511187	43496.499095	32.799104
750.635693	43544.409935	32.804122
750.919477	43600.473479	32.809140
751.740700	43647.391903	32.814157
752.039216	43704.566979	32.819175
753.068828	43760.657416	32.824192
753.754774	43823.291629	32.829210
754.013228	43886.921561	32.834228
754.769385	43953.541882	32.839245
755.629403	44020.016587	32.844263
756.400870	44085.650752	32.849280
757.057868	44151.483199	32.854298
757.974810	44229.148469	32.859316
758.827673	44288.618952	32.864333
759.255693	44360.460345	32.869351
760.104696	44430.727094	32.874368
760.912649	44495.994217	32.879386
761.396657	44572.417603	32.884404
762.723932	44637.574194	32.889421
763.177688	44712.987204	32.894439
763.969725	44778.970885	32.899456
764.728661	44850.723766	32.904474
765.077386	44926.211203	32.909492
766.122783	45003.559783	32.914509
766.737576	45092.110427	32.919527
767.803176	45164.150185	32.924544
768.643914	45229.765022	32.929562
769.252897	45310.490660	32.934580
770.414593	45381.247786	32.939597
770.831322	45454.846411	32.944615
772.003855	45528.937071	32.949632
773.038688	45596.484705	32.954650
773.901064	45666.366263	32.959668
774.775957	45730.857568	32.964685
775.295807	45799.308235	32.969703
776.127507	45860.812900	32.974720
777.009704	45924.126975	32.979738
777.516263	46000.398431	32.984756
778.411737	46056.561801	32.989773
779.286758	46130.156567	32.994791
779.912495	46200.996023	32.999808
780.735782	46274.063285	33.004826
781.239159	46348.396449	33.009844
782.109943	46411.177755	33.014861
782.784694	46492.258046	33.019879
783.623778	46560.534667	33.024896
784.288142	46633.316376	33.029914
784.854216	46711.345119	33.034932
786.115439	46773.977231	33.039949
786.782206	46851.772870	33.044967
787.342808	46926.392793	33.049984
788.284427	46995.383613	33.055002
789.085496	47065.198477	33.060020
789.970200	47123.622893	33.065037
790.128378	47188.224183	33.070055
791.083814	47248.029172	33.075072
792.311264	47318.758425	33.080090
793.136933	47397.594475	33.085108
794.029042	47446.076809	33.090125
794.664434	47524.606110	33.095143
795.470821	47587.660599	33.100160
796.490360	47654.628575	33.105178
796.814360	47714.071840	33.110196
798.124961	47776.696515	33.115213
798.730420	47855.591754	33.120231
799.353773	47914.779798	33.125248
800.082293	47971.897210	33.130266
801.063330	48047.919011	33.135284
801.556970	48113.085570	33.140301
802.408497	48187.992677	33.145319
803.320937	48261.278029	33.150336
804.224945	48332.548760	33.155354
804.905668	48417.723137	33.160372
805.900880	48487.127774	33.165389
806.307336	48562.302944	33.170407
807.144678	48629.764307	33.175424
807.940060	48697.283093	33.180442
808.523199	48791.568703	33.185460
809.613132	48867.381057	33.190477
810.245619	48946.122236	33.195495
810.975775	49024.914483	33.200512
811.866171	49108.260185	33.205530
812.736081	49187.497921	33.210548
813.783149	49268.484367	33.215565
814.470486	49348.654360	33.220583
815.489300	49415.108456	33.225600
816.370360	49494.762320	33.230618
817.057777	49577.303152	33.235636
818.110205	49650.840191	33.240653
818.922738	49730.723754	33.245671
819.516236	49805.697697	33.250688
820.772820	49878.975980	33.255706
821.361410	49954.614013	33.260724
822.251954	50026.748869	33.265741
823.246877	50103.591429	33.270759
823.830143	50172.509673	33.275776
824.867461	50248.673953	33.280794
825.652622	50332.471312	33.285812
826.680739	50400.391855	33.290829
827.726379	50471.383545	33.295847
828.443691	50546.356674	33.300864
829.555424	50603.595126	33.305882
830.298042	50673.553429	33.310900
830.897497	50737.119103	33.315917
831.603213	50808.099965	33.320935
832.193516	50892.328593	33.325952
833.158039	50954.281122	33.330970
833.769532	51025.539775	33.335988
834.374256	51085.467181	33.341005
835.233222	51163.023912	33.346023
835.818035	51229.071003	33.351040
836.689904	51292.645784	33.356058
837.469225	51368.751757	33.361076
838.698781	51439.456081	33.366093
839.127336	51526.976632	33.371111
839.660896	51604.697521	33.376128
841.045973	51671.764474	33.381146
841.522460	51770.576845	33.386164
842.153403	51836.492591	33.391181
843.213727	51919.985324	33.396199
843.937896	52005.068917	33.401216
844.990489	52083.640287	33.406234
845.576455	52176.393701	33.411252
846.402338	52248.670886	33.416269
847.477037	52336.969915	33.421287
848.418008	52425.533679	33.426304
849.551372	52501.477636	33.431322
849.996822	52586.908164	33.436340
850.860484	52667.390029	33.441357
851.925404	52746.502025	33.446375
852.711475	52842.146430	33.451392
853.161152	52918.721720	33.456410
854.414568	53010.274849	33.461428
855.530103	53091.722182	33.466445
856.400384	53182.595458	33.471463
857.044184	53261.233864	33.476480
858.038827	53341.398046	33.481498
859.107578	53424.672313	33.486516
859.999777	53505.207024	33.491533
860.899862	53583.058006	33.496551
861.418863	53671.265779	33.501568
862.594670	53749.723791	33.506586
863.297538	53834.557417	33.511604
864.288826	53910.009114	33.516621
865.406774	53994.723771	33.521639
866.044663	54081.156531	33.526656
866.819961	54161.794827	33.531674
867.593939	54238.270418	33.536692
868.284491	54324.531821	33.541709
869.370051	54421.967611	33.546727
870.319814	54496.235227	33.551744
871.223375	54578.808790	33.556762
871.888765	54660.647299	33.561780
872.636260	54737.804686	33.566797
873.686527	54833.234465	33.571815
874.384172	54932.868510	33.576832
875.671302	55006.992980	33.581850
876.412967	55090.551052	33.586868
877.107294	55186.598032	33.591885
878.339448	55265.688088	33.596903
879.236837	55351.533176	33.601920
880.206735	55422.562714	33.606938
880.781506	55502.926354	33.611956
881.915053	55575.960142	33.616973
882.865490	55645.033384	33.621991
883.282873	55718.879330	33.627008
884.344171	55793.415419	33.632026
884.975325	55867.991857	33.637044
885.924770	55941.690894	33.642061
886.633986	56026.372713	33.647079
887.227783	56107.578815	33.652096
888.117209	56194.480308	33.657114
888.955633	56284.607044	33.662132
889.897916	56379.080330	33.667149
890.506100	56464.433696	33.672167
891.431669	56560.179593	33.677184
892.411205	56643.908931	33.682202
893.416864	56749.789028	33.687220
894.066548	56834.629260	33.692237
894.821516	56924.744004	33.697255
895.596568	57033.194221	33.702272
896.835806	57123.434912	33.707290
897.787385	57230.456543	33.712308
898.776371	57319.696242	33.717325
899.758295	57408.539724	33.722343
900.568590	57500.056467	33.727360
901.856385	57598.275675	33.732378
902.651118	57702.900458	33.737396
903.684760	57791.819636	33.742413
904.792407	57880.342310	33.747431
905.609889	57970.897352	33.752448
906.766392	58051.469995	33.757466
907.869616	58142.416078	33.762484
908.666930	58222.822475	33.767501
909.522229	58312.290295	33.772519
910.258501	58403.103470	33.777536
911.466891	58483.518196	33.782554
912.408466	58584.885397	33.787572
913.506852	58665.956161	33.792589
914.164876	58748.821162	33.797607
914.979703	58840.410109	33.802624
915.776617	58931.986571	33.807642
916.319702	59027.288334	33.812660
917.070208	59116.353639	33.817677
918.487574	59208.647296	33.822695
919.165878	59315.149838	33.827712
920.492101	59402.356837	33.832730
921.499832	59490.022215	33.837748
922.114643	59584.103016	33.842765
923.365957	59677.442073	33.847783
924.074523	59768.386299	33.852800
925.209444	59857.845477	33.857818
925.819176	59958.417320	33.862836
927.131843	60045.901022	33.867853
928.306684	60128.011083	33.872871
928.550557	60220.528057	33.877888
929.508890	60304.116278	33.882906
930.450051	60397.066246	33.887924
930.971596	60484.981003	33.892941
931.564360	60566.241531	33.897959
932.300677	60670.159755	33.902976
933.510441	60758.698822	33.907994
933.900138	60860.573519	33.913012
935.000066	60955.035544	33.918029
936.073389	61050.310610	33.923047
937.052427	61163.741370	33.928064
938.231186	61262.903490	33.933082
938.860109	61354.259626	33.938100
939.726659	61462.200077	33.943117
940.815870	61566.805991	33.948135
941.588265	61666.776944	33.953152
942.915831	61754.787266	33.958170
943.887829	61867.857101	33.963188
944.556319	61976.488812	33.968205
945.889292	62074.879140	33.973223
946.762972	62186.911852	33.978240
947.672470	62284.821210	33.983258
948.686311	62375.303188	33.988276
949.709066	62481.311009	33.993293
950.690235	62595.387917	33.998311
951.587338	62694.832905	34.003328
952.561179	62790.397854	34.008346
953.639210	62894.829752	34.013364
954.269508	63001.518713	34.018381
955.727733	63104.801809	34.023399
956.340587	63202.741008	34.028416
957.374988	63307.257910	34.033434
958.626132	63412.517754	34.038452
959.431742	63523.473396	34.043469
960.129145	63623.015026	34.048487
960.990048	63736.660025	34.053504
962.223749	63839.382824	34.058522
963.231527	63947.880263	34.063540
963.734740	64048.358209	34.068557
965.397970	64151.200675	34.073575
966.159446	64273.517791	34.078592
967.555270	64365.963342	34.083610
968.834293	64466.193729	34.088628
969.811948	64561.132193	34.093645
970.518502	64657.399627	34.098663
971.541140	64759.545129	34.103680
972.611958	64848.608647	34.108698
973.822512	64948.290304	34.113716
974.338607	65043.525672	34.118733
975.658185	65128.735799	34.123751
976.368373	65241.166234	34.128768
977.365006	65342.027260	34.133786
978.110483	65438.677737	34.138804
979.023911	65543.962017	34.143821
980.327543	65640.439433	34.148839
981.023802	65756.725081	34.153856
981.920163	65839.728550	34.158874
983.027836	65931.763239	34.163892
983.769528	66024.320877	34.168909
984.954429	66113.012065	34.173927
985.709367	66220.106593	34.178944
986.335004	66310.653218	34.183962
987.706200	66401.230098	34.188980
988.633974	66503.418924	34.193997
989.678652	66592.785273	34.199015
990.358098	66702.512858	34.204032
991.552939	66802.181369	34.209050
992.782832	66899.406445	34.214068
993.363308	67006.552045	34.219085
994.563902	67108.665927	34.224103
995.677521	67193.099910	34.229120
996.623293	67302.703249	34.234138
997.793755	67399.251725	34.239156
998.893682	67497.681802	34.244173
1000.198524	67585.233053	34.249191
1001.219972	67688.945178	34.254208
1002.010997	67789.700106	34.259226
1002.912813	67878.264398	34.264244
1003.944893	67983.814755	34.269261
1005.000408	68082.905559	34.274279
1005.807474	68190.899774	34.279296
1006.500760	68292.772095	34.284314
1007.439044	68405.819566	34.289332
1008.565699	68513.303547	34.294349
1009.395690	68623.046474	34.299367
1010.419327	68737.769088	34.304384
1011.273491	68851.059958	34.309402
1012.798042	68961.749345	34.314420
1013.670207	69083.005317	34.319437
1014.464497	69185.118940	34.324455
1015.216150	69301.802422	34.329472
1016.720180	69409.679871	34.334490
1017.403303	69531.992191	34.339508
1018.577254	69653.829162	34.344525
1019.854440	69756.418604	34.349543
1020.321974	69885.388642	34.354560
1021.511858	69997.956719	34.359578
1022.687194	70112.814897	34.364596
1023.666394	70232.639391	34.369613
1025.179226	70348.961608	34.374631
1025.944707	70473.218997	34.379648
1027.104082	70583.906149	34.384666
1028.265298	70697.379981	34.389684
1029.185541	70812.074324	34.394701
1030.317668	70928.258344	34.399719
1031.261712	71043.367255	34.404736
1032.181195	71157.393980	34.409754
1033.722276	71260.732777	34.414772
1034.402882	71377.743166	34.419789
1035.443863	71485.048554	34.424807
1036.548445	71596.097622	34.429824
1037.671559	71708.123746	34.434842
1038.646341	71798.374890	34.439860
1039.857284	71908.966493	34.444877
1040.880009	71999.514222	34.449895
1041.533673	72102.417270	34.454912
1042.238712	72209.666289	34.459930
1043.470177	72306.519912	34.464948
1044.073261	72419.966043	34.469965
1045.281423	72518.170312	34.474983
1046.423231	72632.890512	34.480000
1047.091170	72748.198585	34.485018
1047.974332	72861.830164	34.490036
1048.953714	72990.347250	34.495053
1050.058115	73101.240476	34.500071
1051.147743	73228.970643	34.505088
1052.184101	73348.444717	34.510106
1053.096930	73464.766949	34.515124
1054.025035	73596.885369	34.520141
1055.449187	73725.165819	34.525159
1056.332747	73852.503046	34.530176
1057.503794	73974.992685	34.535194
1058.692271	74103.843874	34.540212
1059.575743	74238.766776	34.545229
1060.755914	74359.222473	34.550247
1062.106050	74487.911389	34.555264
1063.270535	74603.125895	34.560282
1064.570514	74726.275802	34.565300
1065.595863	74849.008818	34.570317
1066.607386	74964.894327	34.575335
1067.821792	75089.823243	34.580352
1068.877343	75207.011309	34.585370
1069.910801	75323.078660	34.590388
1070.697875	75450.296006	34.595405
1072.210770	75566.787761	34.600423
1073.241488	75694.467155	34.605440
1074.181674	75814.084956	34.610458
1075.873831	75926.037882	34.615476
1076.719085	76042.423701	34.620493
1077.883193	76157.185796	34.625511
1079.139265	76271.074393	34.630528
1080.018527	76394.067561	34.635546
1080.947841	76507.371134	34.640564
1082.275099	76633.979113	34.645581
1083.226696	76743.216616	34.650599
1084.117746	76864.466394	34.655616
1085.260698	76988.520937	34.660634
1086.665939	77108.306253	34.665652
1087.637773	77238.855184	34.670669
1088.850548	77349.887296	34.675687
1089.712877	77465.886695	34.680704
1090.564995	77590.566320	34.685722
1091.819027	77699.710290	34.690740
1092.773421	77832.022880	34.695757
1093.900966	77960.383731	34.700775
1095.235143	78078.580636	34.705792
1095.890745	78197.556139	34.710810
1097.268910	78309.098096	34.715828
1098.095387	78420.785294	34.720845
1099.196046	78529.996017	34.725863
1100.439745	78640.094759	34.730880
1101.509676	78754.475618	34.735898
1102.621229	78857.119057	34.740916
1103.344530	78989.804563	34.745933
1104.476685	79098.349612	34.750951
1105.231717	79218.832234	34.755968
1106.299366	79349.101263	34.760986
1107.983631	79458.224102	34.766004
1108.664113	79590.307152	34.771021
1109.790656	79719.178526	34.776039
1110.954440	79843.569429	34.781056
1111.896432	79967.705584	34.786074
1113.402294	80101.809827	34.791092
1114.196782	80225.041771	34.796109
1115.505790	80350.796983	34.801127
1116.704880	80470.622087	34.806144
1117.545793	80608.868370	34.811162
1119.082406	80728.634966	34.816180
1120.401065	80863.342844	34.821197
1121.053246	80990.192543	34.826215
1122.372040	81120.401183	34.831232
1123.442199	81251.427732	34.836250
1124.615537	81373.910879	34.841268
1125.647303	81509.964501	34.846285
1126.699920	81641.027902	34.851303
1128.079731	81780.283596	34.856320
1128.742653	81912.567552	34.861338
1130.223978	82046.448037	34.866356
1131.577517	82177.340514	34.871373
1132.078492	82321.917166	34.876391
1133.596476	82453.493269	34.881408
1134.696367	82597.748987	34.886426
1136.003239	82727.078160	34.891444
1137.287565	82862.145801	34.896461
1138.172766	82995.969117	34.901479
1139.899298	83133.231481	34.906496
1141.002065	83270.745675	34.911514
1141.905628	83391.633463	34.916532
1143.334310	83528.838304	34.921549
1144.234129	83652.332946	34.926567
1145.366437	83782.872325	34.931584
1146.314523	83930.347778	34.936602
1147.615906	84045.302585	34.941620
1148.990545	84187.192554	34.946637
1150.132453	84328.608368	34.951655
1151.236860	84446.467088	34.956672
1152.063348	84584.685005	34.961690
1153.815821	84718.191657	34.966708
1154.664973	84850.546665	34.971725
1155.877185	84981.384226	34.976743
1156.960626	85123.048582	34.981760
1157.879438	85240.188830	34.986778
1159.285453	85364.403311	34.991796
1160.301258	85484.899527	34.996813
1161.349865	85610.752989	35.001831
1162.751201	85722.944244	35.006848
1163.814089	85854.405279	35.011866
1165.008989	85974.502734	35.016884
1166.102569	86092.890799	35.021901
1167.333442	86210.473632	35.026919
1168.355239	86341.786130	35.031936
1168.992597	86468.626898	35.036954
1170.771615	86590.114538	35.041972
1171.576913	86730.341546	35.046989
1172.283056	86860.613511	35.052007
1174.056892	86988.787889	35.057024
1175.078865	87129.817724	35.062042
1176.303813	87258.371870	35.067060
1177.825852	87400.721425	35.072077
1178.406606	87531.757238	35.077095
1179.973510	87665.552148	35.082112
1180.993098	87810.273405	35.087130
1182.715640	87937.177933	35.092148
1183.789751	88075.410674	35.097165
1184.683511	88216.594491	35.102183
1186.283643	88342.230852	35.107200
1187.182802	88485.160896	35.112218
1188.592157	88614.104852	35.117236
1190.051923	88754.538189	35.122253
1191.518191	88885.144189	35.127271
1192.339886	89015.594195	35.132288
1193.382247	89156.905967	35.137306
1194.739952	89287.506359	35.142324
1195.964742	89421.549942	35.147341
1196.966853	89550.893076	35.152359
1198.365860	89679.604704	35.157376
1199.489491	89828.395594	35.162394
1200.511117	89960.387853	35.167412
1202.068009	90102.357553	35.172429
1203.297130	90231.807766	35.177447
1204.273118	90372.366430	35.182464
1205.620570	90519.305061	35.187482
1206.749787	90658.500451	35.192500
1207.800611	90799.555907	35.197517
1209.058276	90942.767631	35.202535
1210.585756	91060.171575	35.207552
1211.305206	91205.911833	35.212570
1212.355877	91349.734656	35.217588
1213.803181	91498.346301	35.222605
1214.900086	91637.736457	35.227623
1216.464442	91777.957595	35.232640
1217.780229	91930.387865	35.237658
1219.338759	92061.548448	35.242676
1220.794626	92189.886314	35.247693
1222.064277	92319.475223	35.252711
1223.633097	92445.026349	35.257728
1224.347740	92570.948022	35.262746
1225.580124	92687.136272	35.267764
1226.426131	92800.913511	35.272781
1227.589719	92929.789169	35.277799
1228.868250	93050.361528	35.282816
1230.046349	93174.612716	35.287834
1231.409655	93296.109041	35.292852
1232.419019	93414.297341	35.297869
1233.462236	93554.226780	35.302887
1234.620848	93679.603446	35.307904
1235.718793	93808.425065	35.312922
1236.975351	93946.330601	35.317940
1238.315663	94089.789949	35.322957
1239.261339	94229.062326	35.327975
1240.834168	94356.299851	35.332992
1241.866391	94493.194422	35.338010
1243.295853	94639.046788	35.343028
1244.435165	94779.575880	35.348045
1245.292548	94922.117923	35.353063
1246.798042	95062.375502	35.358080
1248.023721	95205.158093	35.363098
1249.305716	95355.466509	35.368116
1250.723975	95512.858042	35.373133
1251.501156	95655.063248	35.378151
1253.412011	95784.696889	35.383168
1254.874102	95939.497191	35.388186
1256.021631	96075.788454	35.393204
1257.309230	96215.879121	35.398221
1258.348550	96365.758421	35.403239
1259.923326	96502.794059	35.408256
1261.023475	96644.720095	35.413274
1262.187480	96794.512827	35.418292
1263.796751	96937.542734	35.423309
1264.880385	97081.024027	35.428327
1266.530764	97211.339892	35.433344
1267.720833	97363.194575	35.438362
1268.737646	97505.841462	35.443380
1270.239099	97650.183562	35.448397
1271.431301	97794.531459	35.453415
1272.999027	97935.075347	35.458432
1274.225067	98080.191494	35.463450
1274.967713	98224.822357	35.468468
1276.312810	98372.192635	35.473485
1277.484221	98521.514747	35.478503
1279.273564	98661.914003	35.483520
1280.320462	98824.126172	35.488538
1281.703162	98968.470183	35.493556
1283.084578	99103.021556	35.498573
1283.932969	99263.332414	35.503591
1285.374624	99413.749867	35.508608
1286.678098	99564.930511	35.513626
1287.816472	99719.270201	35.518644
1289.141712	99867.228988	35.523661
1290.366956	100022.467975	35.528679
1291.973517	100168.308730	35.533696
1293.072702	100312.143139	35.538714
1293.891934	100456.693618	35.543732
1295.446630	100595.750030	35.548749
1296.529210	100736.932330	35.553767
1297.894571	100883.682762	35.558784
1299.493090	101017.710948	35.563802
1300.690766	101152.967847	35.568820
1301.590053	101293.322162	35.573837
1302.746397	101445.417986	35.578855
1304.360158	101578.118241	35.583872
1305.598491	101739.149880	35.588890
1306.493234	101884.589409	35.593908
1307.988516	102025.365918	35.598925
1309.435865	102191.739511	35.603943
1310.688465	102347.951487	35.608960
1311.785973	102498.304457	35.613978
1313.155481	102655.132663	35.618996
1314.570423	102813.732787	35.624013
1315.522710	102977.355840	35.629031
1317.047025	103128.802989	35.634048
1318.323265	103295.142010	35.639066
1319.485721	103466.708154	35.644084
1321.034834	103617.812804	35.649101
1322.384572	103784.320781	35.654119
1323.707825	103951.966860	35.659136
1325.320915	104115.828168	35.664154
1326.358634	104275.852312	35.669172
1327.765555	104438.172925	35.674189
1329.131685	104614.638338	35.679207
1330.748891	104764.321982	35.684224
1332.070848	104944.600148	35.689242
1333.366005	105112.246249	35.694260
1335.050272	105262.593180	35.699277
1336.132101	105431.471504	35.704295
1337.517033	105595.695722	35.709312
1339.319369	105754.893176	35.714330
1340.282263	105916.997027	35.719348
1341.711444	106074.945919	35.724365
1342.896175	106243.459228	35.729383
1344.279704	106409.309394	35.734400
1345.645596	106569.081609	35.739418
1346.980549	106737.353009	35.744436
1348.403743	106897.061341	35.749453
1349.799527	107057.445949	35.754471
1351.477752	107238.349315	35.759488
1352.833397	107402.001982	35.764506
1354.118829	107548.800186	35.769524
1355.813097	107703.629116	35.774541
1356.997399	107876.103243	35.779559
1358.290596	108019.257532	35.784576
1359.557771	108186.992865	35.789594
1360.505131	108361.735972	35.794612
1362.007439	108512.695481	35.799629
1363.558595	108689.401979	35.804647
1365.017271	108842.104694	35.809664
1366.274205	108999.448205	35.814682
1367.742863	109153.803253	35.819700
1369.329420	109297.424807	35.824717
1370.621116	109449.866721	35.829735
1371.509088	109588.974177	35.834752
1373.178273	109740.047698	35.839770
1374.370935	109892.065043	35.844788
1375.755133	110037.008016	35.849805
1376.907084	110186.938557	35.854823
1378.338365	110346.079646	35.859840
1379.639414	110507.419899	35.864858
1380.615272	110664.014916	35.869876
1382.227214	110818.370353	35.874893
1383.533800	110988.112560	35.879911
1385.163245	111149.461800	35.884928
1386.574223	111312.872402	35.889946
1387.683020	111489.314934	35.894964
1388.969442	111646.328920	35.899981
1390.573381	111807.401661	35.904999
1391.970604	111979.358132	35.910016
1393.199039	112155.526863	35.915034
1394.942758	112332.285953	35.920052
1396.572025	112499.094336	35.925069
1397.655303	112670.972555	35.930087
1398.803602	112832.953633	35.935104
1400.465718	112999.019496	35.940122
1401.780400	113187.158907	35.945140
1403.371555	113343.692055	35.950157
1404.905135	113526.766511	35.955175
1406.266511	113709.293593	35.960192
1407.549633	113877.805816	35.965210
1409.064883	114056.512608	35.970228
1410.689380	114220.300860	35.975245
1412.093837	114403.959339	35.980263
1413.508288	114568.783498	35.985280
1415.141499	114743.006893	35.990298
1416.361381	114917.626382	35.995316
1417.882279	115090.420255	36.000333
1419.258533	115265.504778	36.005351
1420.639733	115432.498713	36.010368
1422.225197	115606.083553	36.015386
1423.602631	115772.637155	36.020404
1425.237903	115938.986267	36.025421
1426.511402	116123.627710	36.030439
1428.162689	116302.335093	36.035456
1429.805541	116469.686802	36.040474
1431.012122	116646.713513	36.045492
1432.244060	116810.751846	36.050509
1433.745145	116984.739376	36.055527
1435.372924	117158.309077	36.060544
1436.978093	117332.700307	36.065562
1438.085960	117505.076019	36.070580
1439.744806	117670.090383	36.075597
1441.058429	117843.758965	36.080615
1442.296746	118009.443833	36.085632
1444.304209	118168.232657	36.090650
1445.395881	118338.596722	36.095668
1446.785688	118482.466814	36.100685
1448.491619	118637.064170	36.105703
1449.632359	118789.548789	36.110720
1451.086960	118948.132668	36.115738
1452.032960	119114.295306	36.120756
1453.819393	119260.468498	36.125773
1455.315490	119417.623969	36.130791
1456.334526	119589.717436	36.135808
1457.756095	119747.640253	36.140826
1458.904220	119938.040484	36.145844
1460.587421	120105.016793	36.150861
1461.959311	120285.594512	36.155879
1463.378756	120456.756230	36.160896
1464.986674	120636.222387	36.165914
1466.249058	120813.553697	36.170932
1467.798386	120983.279779	36.175949
1469.417940	121179.921156	36.180967
1470.465282	121356.429093	36.185984
1472.462875	121534.585649	36.191002
1473.735882	121724.459738	36.196020
1475.290443	121900.662753	36.201037
1476.957302	122089.020391	36.206055
1478.442374	122277.572904	36.211072
1480.191646	122446.529382	36.216090
1481.391318	122636.662312	36.221108
1483.356758	122817.302394	36.226125
1485.046397	122984.333937	36.231143
1486.665858	123164.727378	36.236160
1488.213615	123334.126825	36.241178
1489.754274	123505.631016	36.246196
1491.113654	123685.208020	36.251213
1492.588261	123857.636918	36.256231
1494.063385	124034.272010	36.261248
1495.450260	124211.327608	36.266266
1496.812096	124395.342168	36.271284
1498.550953	124565.593023	36.276301
1499.824232	124759.820611	36.281319
1500.958119	124950.094436	36.286336
1502.796775	125128.591615	36.291354
1504.077171	125310.864700	36.296372
1505.761246	125495.443577	36.301389
1507.372155	125681.770708	36.306407
1508.720528	125868.406840	36.311424
1510.205659	126054.363837	36.316442
1511.918877	126240.805224	36.321460
1513.785106	126426.146860	36.326477
1515.421801	126609.537451	36.331495
1516.607273	126788.858707	36.336512
1517.981534	126975.498315	36.341530
1519.610154	127160.046632	36.346548
1521.496443	127338.120062	36.351565
1522.835644	127522.767475	36.356583
1524.266881	127704.437226	36.361600
1526.193323	127886.903592	36.366618
1527.455879	128050.689947	36.371636
1528.951284	128217.708654	36.376653
1530.280886	128378.572641	36.381671
1531.426164	128535.907070	36.386688
1533.411295	128700.329913	36.391706
1534.414068	128870.800610	36.396724
1536.114078	129043.036523	36.401741
1537.221004	129221.347290	36.406759
1538.819559	129401.595412	36.411776
1540.660244	129578.499699	36.416794
1541.806225	129770.895415	36.421812
1543.457843	129945.893744	36.426829
1544.964615	130133.825870	36.431847
1546.178962	130312.645983	36.436864
1548.112451	130502.945260	36.441882
1549.349142	130695.104880	36.446900
1550.862245	130881.001269	36.451917
1552.489995	131078.080428	36.456935
1554.087162	131281.209176	36.461952
1555.715180	131476.086587	36.466970
1557.210320	131673.190976	36.471988
1558.425670	131856.265086	36.477005
1560.073756	132059.289986	36.482023
1561.567427	132275.454258	36.487040
1563.120809	132476.862770	36.492058
1564.842067	132678.930228	36.497076
1566.739804	132886.622002	36.502093
1568.433657	133087.480374	36.507111
1569.802997	133289.924828	36.512128
1571.523328	133486.714606	36.517146
1573.316056	133696.696972	36.522164
1574.705971	133893.491352	36.527181
1576.801628	134093.152598	36.532199
1578.401210	134294.351181	36.537216
1579.890303	134486.775101	36.542234
1581.726276	134686.025561	36.547252
1583.087628	134889.014737	36.552269
1584.800235	135081.660541	36.557287
1586.298930	135281.374161	36.562304
1587.988568	135476.002955	36.567322
1589.535676	135689.295385	36.572340
1591.087227	135879.133666	36.577357
1592.520737	136080.928595	36.582375
1594.274644	136288.148203	36.587392
1596.027694	136483.052436	36.592410
1597.505077	136691.687383	36.597428
1599.540488	136890.135620	36.602445
1601.130207	137080.051675	36.607463
1602.404861	137286.898283	36.612480
1604.301898	137476.679381	36.617498
1605.801267	137682.568004	36.622516
1607.493374	137872.624978	36.627533
1609.381746	138075.033006	36.632551
1610.483832	138275.995913	36.637568
1612.376547	138452.655203	36.642586
1613.855869	138640.659923	36.647604
1615.513512	138809.869104	36.652621
1616.733227	138988.476033	36.657639
1618.405652	139172.588221	36.662656
1620.294460	139355.970162	36.667674
1621.275739	139545.238288	36.672692
1622.700927	139739.088161	36.677709
1624.619916	139922.772941	36.682727
1625.452308	140111.751461	36.687744
1627.446970	140313.055230	36.692762
1629.089204	140513.960078	36.697780
1630.797792	140713.677083	36.702797
1632.503948	140900.354587	36.707815
1634.023579	141108.354775	36.712832
1635.759179	141296.424163	36.717850
1637.130421	141515.781128	36.722868
1638.918663	141724.718776	36.727885
1640.630917	141937.712967	36.732903
1642.109889	142145.397191	36.737920
1643.901716	142344.668119	36.742938
1645.679982	142565.767747	36.747956
1647.468036	142775.181575	36.752973
1649.197060	142972.882265	36.757991
1650.676022	143190.054132	36.763008
1652.527413	143395.494977	36.768026
1654.208205	143612.371600	36.773044
1655.779942	143821.307243	36.778061
1657.495295	144029.967991	36.783079
1659.122947	144242.408565	36.788096
1660.921739	144443.301717	36.793114
1662.660361	144659.656817	36.798132
1664.312618	144875.900385	36.803149
1666.159382	145084.319196	36.808167
1667.704517	145307.097920	36.813184
1669.459166	145520.427009	36.818202
1671.269281	145719.919606	36.823220
1672.664870	145934.056398	36.828237
1674.343875	146145.373635	36.833255
1676.154858	146365.392357	36.838272
1677.905835	146581.986950	36.843290
1679.850588	146795.002954	36.848308
1681.702540	147000.264640	36.853325
1683.115328	147208.398852	36.858343
1684.715598	147427.457006	36.863360
1686.638430	147640.938526	36.868378
1688.606841	147848.126695	36.873396
1690.045772	148064.590821	36.878413
1691.674073	148268.641232	36.883431
1693.657837	148478.150884	36.888448
1695.295561	148691.595969	36.893466
1696.794051	148900.538925	36.898484
1698.594515	149114.024359	36.903501
1700.063354	149320.135100	36.908519
1701.915432	149541.196064	36.913536
1703.870562	149736.583420	36.918554
1705.463954	149932.320978	36.923572
1706.868262	150120.191726	36.928589
1708.876998	150305.279957	36.933607
1710.169498	150506.101712	36.938624
1711.693084	150699.040560	36.943642
1713.513148	150889.372576	36.948660
1714.935417	151086.196499	36.953677
1716.832035	151284.835281	36.958695
1718.279366	151500.268799	36.963712
1720.233425	151699.534869	36.968730
1721.603197	151905.208615	36.973748
1723.415688	152111.586713	36.978765
1725.320055	152318.560068	36.983783
1726.737886	152540.952754	36.988800
1728.073782	152746.510333	36.993818
1729.785081	152965.968594	36.998836
1731.820677	153192.920563	37.003853
1733.683254	153409.365584	37.008871
1735.052462	153629.795404	37.013888
1736.924853	153846.355809	37.018906
1738.901290	154074.908024	37.023924
1740.431724	154306.474143	37.028941
1742.463165	154530.050556	37.033959
1744.139209	154754.154016	37.038976
1746.178543	154968.970785	37.043994
1747.936476	155204.513596	37.049012
1749.865717	155425.322715	37.054029
1752.194384	155637.422433	37.059047
1753.535339	155863.082620	37.064064
1755.331574	156090.459847	37.069082
1757.319112	156307.613696	37.074100
1758.941344	156519.742318	37.079117
1760.454857	156750.617741	37.084135
1762.183318	156973.345391	37.089152
1764.223076	157187.351888	37.094170
1765.974892	157407.707470	37.099188
1767.980878	157642.530296	37.104205
1770.276009	157849.412105	37.109223
1771.828088	158078.616499	37.114240
1773.754193	158297.910289	37.119258
1775.389227	158511.482024	37.124276
1776.993561	158732.452752	37.129293
1779.092261	158943.277903	37.134311
1780.859670	159167.674649	37.139328
1782.772828	159380.700312	37.144346
1784.287825	159602.946128	37.149364
1786.182753	159823.788840	37.154381
1788.280433	160036.396071	37.159399
1789.553816	160258.785834	37.164416
1791.439044	160479.532741	37.169434
1793.368244	160697.712413	37.174452
1795.060286	160918.530769	37.179469
1796.891152	161132.898937	37.184487
1798.671720	161357.637228	37.189504
1800.546089	161563.352243	37.194522
1802.428412	161756.436185	37.199540
1803.738527	161962.560118	37.204557
1805.777777	162157.244576	37.209575
1807.233276	162356.334619	37.214592
1808.913931	162561.134965	37.219610
1811.255371	162769.230367	37.224628
1812.453338	162979.461550	37.229645
1814.276137	163174.122451	37.234663
1816.171143	163384.980898	37.239680
1817.981638	163591.529298	37.244698
1819.750727	163804.908594	37.249716
1821.258795	164029.656059	37.254733
1823.243991	164241.405602	37.259751
1824.843751	164457.212596	37.264768
1826.175768	164684.604653	37.269786
1828.469688	164911.731270	37.274804
1829.936335	165146.562304	37.279821
1832.060909	165372.386937	37.284839
1833.795781	165603.107056	37.289856
1835.680853	165848.124027	37.294874
1837.542878	166082.720664	37.299892
1838.945088	166316.503941	37.304909
1841.159602	166547.420123	37.309927
1843.199152	166792.317308	37.314944
1844.822884	167035.620555	37.319962
1847.087149	167270.274939	37.324980
1849.064991	167508.717943	37.329997
1851.022026	167747.026235	37.335015
1852.856053	167985.228715	37.340032
1854.974010	168217.946213	37.345050
1856.792282	168462.077585	37.350068
1858.664938	168696.600028	37.355085
1860.909605	168927.132768	37.360103
1862.814191	169152.545707	37.365120
1864.712014	169383.275777	37.370138
1866.914134	169611.282522	37.375156
1868.714264	169848.347719	37.380173
1870.653269	170069.676171	37.385191
1872.614800	170304.803183	37.390208
1874.157071	170527.858914	37.395226
1876.138433	170755.412746	37.400244
1877.844989	170996.406726	37.405261
1879.695207	171213.798118	37.410279
1881.622170	171449.280022	37.415296
1883.517854	171680.582233	37.420314
1885.606446	171908.836123	37.425332
1887.194304	172160.093009	37.430349
1889.118220	172386.067090	37.435367
1891.041523	172621.099914	37.440384
1893.128454	172847.710395	37.445402
1895.129793	173078.420492	37.450420
1896.922795	173315.101850	37.455437
1898.839805	173545.548952	37.460455
1900.780787	173785.748911	37.465472
1902.438831	174009.338741	37.470490
1904.747261	174215.992425	37.475508
1906.343290	174430.371806	37.480525
1908.320603	174635.608627	37.485543
1909.996579	174844.624022	37.490560
1911.620832	175045.580321	37.495578
1913.562989	175265.643325	37.500596
1914.948269	175486.620510	37.505613
1917.085863	175699.284114	37.510631
1919.053091	175935.610645	37.515648
1920.740527	176153.612918	37.520666
1922.935662	176380.023073	37.525684
1924.629922	176617.627448	37.530701
1926.702699	176835.432622	37.535719
1928.512170	177081.458030	37.540736
1930.245434	177322.917042	37.545754
1932.550991	177553.984859	37.550772
1934.389638	177805.084683	37.555789
1936.381406	178041.355918	37.560807
1937.965552	178276.234157	37.565824
1939.814832	178531.256970	37.570842
1942.123645	178776.325008	37.575860
1944.122102	179020.073491	37.580877
1945.931130	179255.961864	37.585895
1948.106887	179501.829157	37.590912
1950.056417	179752.034860	37.595930
1952.304219	179996.497945	37.600948
1954.073610	180249.691374	37.605965
1956.229472	180479.251057	37.610983
1958.648615	180720.646017	37.616000
1960.054882	180968.483594	37.621018
1962.356982	181218.692654	37.626036
1964.812327	181458.309676	37.631053
1966.507262	181698.264392	37.636071
1968.740555	181935.914562	37.641088
1970.601548	182182.608410	37.646106
1972.564966	182408.580007	37.651124
1974.644806	182658.591532	37.656141
1977.034823	182889.890490	37.661159
1978.995484	183121.436436	37.666176
1980.940749	183365.154427	37.671194
1982.852935	183594.312391	37.676212
1984.964040	183831.446576	37.681229
1987.293105	184064.525081	37.686247
1989.135809	184299.521870	37.691264
1991.194134	184531.516462	37.696282
1993.348660	184748.511261	37.701300
1995.098973	184999.146553	37.706317
1997.275153	185223.893238	37.711335
1999.153103	185449.284756	37.716352
2000.931319	185677.687889	37.721370
2003.121157	185914.884014	37.726388
2005.251519	186146.393268	37.731405
2007.535613	186380.328370	37.736423
2009.489375	186601.894030	37.741440
2011.272312	186827.726189	37.746458
2013.224349	187033.318009	37.751476
2015.094416	187246.118814	37.756493
2017.005433	187446.719239	37.761511
2019.252231	187654.690796	37.766528
2020.762922	187860.559356	37.771546
2022.875989	188069.543798	37.776564
2024.820881	188294.951329	37.781581
2026.437063	188507.315966	37.786599
2028.665990	188722.071603	37.791616
2030.026426	188957.168769	37.796634
2032.706728	189174.849734	37.801652
2034.287463	189402.477688	37.806669
2036.084566	189642.876968	37.811687
2038.202832	189868.036079	37.816704
2040.139986	190109.265750	37.821722
2042.423464	190346.342644	37.826740
2044.161074	190588.647014	37.831757
2046.512964	190832.390712	37.836775
2048.611429	191074.119953	37.841792
2050.744256	191319.880623	37.846810
2053.344213	191552.230333	37.851828
2055.403600	191803.525625	37.856845
2057.316349	192038.550251	37.861863
2059.914317	192271.627092	37.866880
2061.739458	192519.930067	37.871898
2063.800924	192750.847974	37.876916
2066.072103	192985.414145	37.881933
2068.427527	193223.178959	37.886951
2070.647371	193451.574826	37.891968
2072.545531	193684.769361	37.896986
2075.217929	193910.798392	37.902004
2077.327237	194138.694591	37.907021
2079.213796	194366.576397	37.912039
2081.731045	194588.724093	37.917056
2083.569175	194817.834019	37.922074
2086.119886	195041.729852	37.927092
2088.147144	195266.534684	37.932109
2090.105722	195480.842547	37.937127
2092.319396	195693.625889	37.942144
2094.495182	195932.104659	37.947162
2096.669422	196148.691045	37.952180
2098.711216	196368.548524	37.957197
2100.906257	196589.233001	37.962215
2103.442014	196799.558320	37.967232
2105.483539	197021.855517	37.972250
2107.502613	197233.368781	37.977268
2109.487743	197447.769448	37.982285
2111.685114	197658.976921	37.987303
2114.123783	197869.080802	37.992320
2115.919911	198095.267296	37.997338
2118.168138	198298.117609	38.002356
2120.421062	198508.862747	38.007373
2122.589961	198722.998294	38.012391
2124.662389	198937.568866	38.017408
2126.701903	199139.757405	38.022426
2128.823617	199328.974335	38.027444
2130.536488	199509.041792	38.032461
2132.562818	199705.180077	38.037479
2134.407096	199888.096548	38.042496
2136.544017	200096.835476	38.047514
2138.355920	200286.523781	38.052532
2140.688240	200492.783488	38.057549
2142.390986	200700.273528	38.062567
2144.459966	200904.355270	38.067584
2146.311795	201109.119571	38.072602
2148.859495	201324.512745	38.077620
2150.629116	201544.257049	38.082637
2152.713017	201760.207838	38.087655
2154.967456	201977.681013	38.092672
2157.045094	202210.085194	38.097690
2159.301214	202429.489273	38.102708
2161.360148	202659.803864	38.107725
2163.521889	202885.216057	38.112743
2165.712255	203112.185931	38.117760
2167.817957	203345.339289	38.122778
2170.187427	203570.911677	38.127796
2172.252460	203812.197409	38.132813
2174.532991	204049.870312	38.137831
2176.977383	204288.013276	38.142848
2178.978151	204527.738173	38.147866
2181.197374	204753.148646	38.152884
2183.557375	204990.952471	38.157901
2185.696494	205231.267658	38.162919
2187.975481	205467.905731	38.167936
2190.048861	205715.062806	38.172954
2192.389793	205939.620755	38.177972
2194.530805	206179.165186	38.182989
2196.821219	206423.041067	38.188007
2199.429818	206659.263526	38.193024
2201.465252	206900.617536	38.198042
2203.780874	207145.761836	38.203060
2206.035689	207380.240639	38.208077
2208.002311	207618.790262	38.213095
2210.242092	207858.706618	38.218112
2212.549601	208098.930554	38.223130
2214.745226	208349.760635	38.228148
2217.015139	208594.080212	38.233165
2219.371522	208834.007315	38.238183
2221.401907	209065.417976	38.243200
2223.711718	209313.060161	38.248218
2225.719202	209561.195611	38.253236
2228.288678	209790.251082	38.258253
2230.170717	210039.639758	38.263271
2232.857047	210294.424285	38.268288
2234.992123	210523.424382	38.273306
2237.440872	210776.052265	38.278324
2239.728731	211019.984980	38.283341
2241.609407	211266.712711	38.288359
2244.079825	211486.078102	38.293376
2246.198939	211733.937806	38.298394
2248.302170	211961.640503	38.303412
2250.274314	212174.117427	38.308429
2252.369501	212393.532726	38.313447
2254.638537	212610.889897	38.318464
2256.486742	212845.415618	38.323482
2258.809775	213072.744579	38.328500
2260.979160	213299.692429	38.333517
2262.859220	213543.470816	38.338535
2265.287680	213771.521833	38.343552
2267.471093	214017.297897	38.348570
2269.383387	214266.647337	38.353588
2271.776415	214515.515204	38.358605
2273.984286	214770.558245	38.363623
2276.492837	215016.045192	38.368640
2278.658385	215281.698119	38.373658
2280.997277	215528.648490	38.378676
2283.327932	215793.134573	38.383693
2285.340839	216050.714491	38.388711
2288.071180	216303.572842	38.393728
2290.432806	216570.608965	38.398746
2292.522792	216825.107018	38.403764
2295.043925	217072.668841	38.408781
2297.287660	217356.955790	38.413799
2299.758511	217610.977320	38.418816
2302.051609	217877.369065	38.423834
2304.116487	218148.990932	38.428852
2306.749386	218407.230304	38.433869
2308.795716	218687.732161	38.438887
2311.838488	218948.358967	38.443904
2314.093809	219211.803298	38.448922
2316.329238	219481.117708	38.453940
2318.948351	219740.659107	38.458957
2320.916211	220008.710092	38.463975
2323.588003	220270.314618	38.468992
2325.784601	220536.947271	38.474010
2327.842466	220786.093532	38.479028
2330.462943	221056.406487	38.484045
2332.791567	221340.327317	38.489063
2335.744909	221605.650249	38.494080
2337.948688	221879.193830	38.499098
2340.113723	222145.354671	38.504116
2342.528507	222406.956565	38.509133
2344.878909	222680.682912	38.514151
2347.133915	222932.395212	38.519168
2349.292598	223206.547426	38.524186
2351.955390	223470.830851	38.529204
2354.350623	223744.922047	38.534221
2356.424908	224016.703308	38.539239
2359.059262	224305.576697	38.544256
2361.256410	224613.503577	38.549274
2363.320865	224890.368459	38.554292
2365.874767	225159.677668	38.559309
2367.992947	225432.650342	38.564327
2370.592459	225700.404962	38.569344
2373.056626	225974.822944	38.574362
2375.219671	226226.814107	38.579380
2377.583185	226468.488841	38.584397
2379.306388	226721.008352	38.589415
2381.747986	226968.081529	38.594432
2383.977600	227216.814397	38.599450
2385.963115	227483.389548	38.604468
2388.649663	227744.673524	38.609485
2390.736195	228019.361196	38.614503
2393.362438	228280.402392	38.619520
2395.623929	228559.178291	38.624538
2397.851358	228829.071608	38.629556
2400.405763	229096.171062	38.634573
2402.653445	229382.951770	38.639591
2405.027588	229655.491029	38.644608
2407.613946	229946.816721	38.649626
2409.471161	230235.414452	38.654644
2412.155335	230521.647057	38.659661
2414.554667	230808.738426	38.664679
2416.834220	231101.310121	38.669696
2419.179853	231392.475406	38.674714
2421.803401	231693.451805	38.679732
2424.393742	231996.745622	38.684749
2426.646153	232296.995454	38.689767
2429.348821	232601.340106	38.694784
2432.094467	232900.599335	38.699802
2434.191634	233205.854610	38.704820
2437.213864	233506.468762	38.709837
2439.626385	233811.142588	38.714855
2442.046029	234106.342696	38.719872
2444.611338	234405.101751	38.724890
2447.055138	234704.439722	38.729908
2449.640430	235000.555954	38.734925
2452.008194	235312.200616	38.739943
2454.804700	235603.840387	38.744960
2457.414572	235907.295539	38.749978
2459.778747	236208.987211	38.754996
2462.406360	236500.707069	38.760013
2464.937301	236805.320283	38.765031
2467.372502	237100.170952	38.770048
2469.743775	237407.630474	38.775066
2472.024078	237705.580633	38.780084
2474.804852	238002.360125	38.785101
2477.073983	238315.502410	38.790119
2479.586153	238612.148321	38.795136
2482.009320	238918.791075	38.800154
2484.353113	239228.952365	38.805172
2486.885163	239533.801572	38.810189
2489.382380	239837.158537	38.815207
2491.685643	240149.589306	38.820224
2494.283833	240466.901714	38.825242
2496.932433	240770.389518	38.830260
2499.626261	241072.905738	38.835277
2502.183061	241393.198965	38.840295
2504.597964	241706.149541	38.845312
2507.185759	241997.127901	38.850330
2509.187531	242289.520624	38.855348
2511.822999	242555.270467	38.860365
2513.915929	242843.992426	38.865383
2516.493730	243122.909911	38.870400
2519.045179	243408.715667	38.875418
2520.791728	243703.819142	38.880436
2523.547492	243986.367954	38.885453
2525.633622	244293.814357	38.890471
2528.298205	244593.448046	38.895488
2530.717149	244894.162758	38.900506
2532.872634	245213.563967	38.905524
2535.900915	245517.917401	38.910541
2537.933361	245833.275439	38.915559
2540.381056	246150.702059	38.920576
2542.954950	246483.222922	38.925594
2545.586084	246812.839784	38.930612
2548.208388	247135.295720	38.935629
2550.675499	247472.357166	38.940647
2553.335614	247802.682907	38.945664
2556.083128	248136.297683	38.950682
2558.686808	248480.426693	38.955700
2561.282110	248808.580400	38.960717
2563.855122	249152.461760	38.965735
2566.244326	249486.771273	38.970752
2569.081718	249823.398209	38.975770
2571.755020	250171.838142	38.980788
2574.499558	250494.942190	38.985805
2576.936646	250845.148283	38.990823
2579.631956	251193.002643	38.995840
2582.299954	251534.816436	39.000858
2584.799840	251882.626953	39.005876
2587.632027	252224.644702	39.010893
2590.677018	252576.917141	39.015911
2593.131922	252913.737801	39.020928
2595.791224	253260.408049	39.025946
2598.265914	253604.288572	39.030964
2600.922097	253942.095279	39.035981
2603.530792	254296.294445	39.040999
2606.006151	254638.144542	39.046016
2608.987503	254971.837170	39.051034
2611.529079	255327.318915	39.056052
2614.076757	255667.381139	39.061069
2616.810442	256020.826856	39.066087
2619.555259	256364.999544	39.071104
2622.438620	256707.575880	39.076122
2624.509600	257058.003787	39.081140
2627.388779	257395.831591	39.086157
2630.299444	257741.707493	39.091175
2632.822703	258101.210230	39.096192
2635.362795	258437.162664	39.101210
2638.028378	258781.300719	39.106228
2640.987721	259130.092197	39.111245
2643.347838	259481.316129	39.116263
2645.980893	259820.583430	39.121280
2648.977575	260151.232837	39.126298
2650.915620	260483.599924	39.131316
2653.802658	260790.414281	39.136333
2656.046032	261111.861347	39.141351
2658.522643	261438.377792	39.146368
2661.276360	261752.301679	39.151386
2663.315773	262075.865132	39.156404
2666.009502	262400.773234	39.161421
2668.482614	262746.648644	39.166439
2671.105996	263078.224142	39.171456
2674.085918	263419.523639	39.176474
2676.385677	263776.198434	39.181492
2679.179351	264117.121661	39.186509
2681.560512	264472.590299	39.191527
2684.371100	264821.843694	39.196544
2686.765522	265184.271328	39.201562
2689.325658	265555.945179	39.206580
2692.151732	265915.155082	39.211597
2694.485416	266297.890409	39.216615
2697.183072	266667.282525	39.221632
2700.413900	267037.911438	39.226650
2702.708435	267424.515148	39.231668
2705.714809	267807.576948	39.236685
2708.673784	268181.221905	39.241703
2711.408778	268559.576783	39.246720
2714.387508	268947.292507	39.251738
2717.339387	269330.744956	39.256756
2720.000508	269708.680339	39.261773
2722.524206	270086.536064	39.266791
2725.218779	270469.648798	39.271808
2728.448131	270846.097526	39.276826
2730.599079	271235.774544	39.281844
2733.759889	271633.674873	39.286861
2736.947422	272011.858075	39.291879
2739.669937	272403.172385	39.296896
2742.568617	272776.752724	39.301914
2744.665520	273169.207846	39.306932
2748.098973	273550.731116	39.311949
2750.663437	273938.412685	39.316967
2753.416090	274325.200775	39.321984
2756.389382	274706.390602	39.327002
2758.947726	275098.595036	39.332020
2761.842681	275477.866626	39.337037
2764.806333	275859.566053	39.342055
2767.466549	276261.687050	39.347072
2770.280394	276643.333924	39.352090
2773.075614	277040.149528	39.357108
2775.835353	277430.721441	39.362125
2778.445317	277804.169695	39.367143
2781.268199	278201.920585	39.372160
2783.983565	278598.646844	39.377178
2786.840381	278995.884039	39.382196
2789.910104	279393.061964	39.387213
2792.645833	279772.992936	39.392231
2795.355121	280167.407833	39.397248
2798.616068	280538.135488	39.402266
2801.027224	280912.985855	39.407284
2803.851733	281254.568451	39.412301
2806.339528	281610.506245	39.417319
2808.720523	281971.795436	39.422336
2812.023426	282326.435186	39.427354
2814.092011	282697.858489	39.432372
2816.471883	283069.841919	39.437389
2819.457267	283444.980805	39.442407
2821.745863	283818.273696	39.447424
2824.868293	284200.757213	39.452442
2827.621255	284593.307745	39.457460
2830.682043	284980.474522	39.462477
2833.520449	285366.507609	39.467495
2836.029060	285767.580351	39.472512
2839.415484	286154.567409	39.477530
2841.741205	286548.580831	39.482548
2844.365604	286955.476641	39.487565
2847.466940	287367.631071	39.492583
2850.313775	287785.312318	39.497600
2852.892592	288196.405310	39.502618
2855.785955	288610.801131	39.507636
2858.620157	289034.757208	39.512653
2861.306134	289459.142587	39.517671
2864.287644	289884.979300	39.522688
2867.398340	290311.887218	39.527706
2870.544026	290737.264759	39.532724
2873.626456	291170.272406	39.537741
2876.574694	291598.728101	39.542759
2879.380795	292016.485693	39.547776
2882.568169	292441.802941	39.552794
2885.096488	292872.786899	39.557812
2888.106880	293299.578538	39.562829
2891.376290	293727.496863	39.567847
2894.247639	294165.943117	39.572864
2897.708997	294589.612573	39.577882
2900.282425	295007.858673	39.582900
2903.217960	295447.740007	39.587917
2906.402276	295889.257528	39.592935
2909.195477	296310.031728	39.597952
2912.199242	296730.822476	39.602970
2915.042378	297162.611337	39.607988
2917.906429	297592.262125	39.613005
2921.009789	298034.803515	39.618023
2923.514540	298472.612246	39.623040
2926.752167	298901.819707	39.628058
2929.754677	299346.456675	39.633076
2932.702361	299775.250602	39.638093
2935.829570	300212.295870	39.643111
2938.762274	300633.291680	39.648128
2941.835142	301068.285719	39.653146
2944.513642	301505.474688	39.658164
2947.563267	301942.679874	39.663181
2950.577105	302377.806579	39.668199
2953.484005	302810.840662	39.673216
2956.425458	303231.116726	39.678234
2959.351800	303634.273774	39.683252
2961.819867	304035.444764	39.688269
2964.730654	304429.762537	39.693287
2967.308633	304842.598154	39.698304
2970.184219	305237.782816	39.703322
2972.794296	305656.072013	39.708340
2975.930424	306071.711189	39.713357
2978.714712	306485.779124	39.718375
2981.367599	306901.542957	39.723392
2984.298954	307333.720681	39.728410
2987.050649	307774.256597	39.733428
2989.771768	308222.339597	39.738445
2993.179109	308657.815597	39.743463
2995.803653	309119.499547	39.748480
2998.560175	309566.276599	39.753498
3001.663759	310034.078712	39.758516
3004.579832	310498.911487	39.763533
3007.864286	310958.147011	39.768551
3010.472763	311431.482689	39.773568
3013.636286	311903.610957	39.778586
3017.059397	312369.473352	39.783604
3019.886050	312849.930984	39.788621
3023.177860	313319.950123	39.793639
3026.387880	313803.644664	39.798656
3029.412763	314280.102279	39.803674
3032.426405	314757.397644	39.808692
3035.595556	315244.419165	39.813709
3038.891219	315711.734669	39.818727
3042.059711	316202.510621	39.823744
3045.103366	316683.093897	39.828762
3048.369007	317163.030138	39.833780
3051.308816	317643.117161	39.838797
3054.612919	318120.223397	39.843815
3057.542482	318612.294850	39.848832
3061.048907	319092.995990	39.853850
3064.088719	319570.695414	39.858868
3066.841008	320057.555418	39.863885
3070.685616	320534.411314	39.868903
3073.582484	321020.760699	39.873920
3076.576477	321502.469850	39.878938
3079.761274	321973.758970	39.883956
3082.737379	322457.700588	39.888973
3086.127262	322940.989894	39.893991
3088.925766	323429.474667	39.899008
3092.012638	323912.196881	39.904026
3095.241051	324393.293970	39.909044
3098.128354	324873.045477	39.914061
3101.516981	325355.102026	39.919079
3104.551380	325853.794955	39.924096
3107.700830	326349.596923	39.929114
3111.076157	326826.466123	39.934132
3113.960447	327316.361549	39.939149
3117.293976	327799.707152	39.944167
3120.601624	328285.999605	39.949184
3123.475469	328747.496455	39.954202
3126.672568	329199.441886	39.959220
3129.579311	329646.453299	39.964237
3132.677038	330089.775085	39.969255
3135.521966	330533.997610	39.974272
3138.298202	330973.809820	39.979290
3141.110298	331431.566933	39.984308
3144.135474	331895.483418	39.989325
3147.117957	332353.893335	39.994343
3150.134459	332834.310680	39.999360
3153.032307	333298.136599	40.004378
3156.207351	333788.400166	40.009396
3158.781374	334279.796458	40.014413
3161.981206	334776.041734	40.019431
3165.230377	335271.107561	40.024448
3168.209618	335781.650781	40.029466
3171.406692	336288.092977	40.034484
3174.453583	336803.721436	40.039501
3177.764254	337308.436637	40.044519
3180.768251	337834.042611	40.049536
3184.136486	338357.276132	40.054554
3187.316887	338873.273368	40.059572
3190.509216	339407.114099	40.064589
3193.866237	339925.131498	40.069607
3197.095643	340463.959320	40.074624
3200.274015	341003.628425	40.079642
3203.799582	341532.929691	40.084660
3206.834826	342068.041974	40.089677
3210.209962	342607.005722	40.094695
3213.454093	343156.826482	40.099712
3216.982533	343690.500745	40.104730
3220.409041	344224.897219	40.109748
3223.648175	344777.039522	40.114765
3227.124751	345309.336366	40.119783
3230.438326	345854.474966	40.124800
3233.917289	346381.557059	40.129818
3237.158310	346912.530809	40.134836
3240.337618	347454.222714	40.139853
3243.736637	347992.295106	40.144871
3246.992119	348538.178715	40.149888
3250.641197	349070.159123	40.154906
3253.656516	349611.449804	40.159924
3256.847914	350149.914830	40.164941
3260.223579	350685.730650	40.169959
3263.245034	351219.337874	40.174976
3266.678224	351762.495608	40.179994
3270.321095	352306.630019	40.185012
3273.508646	352852.201605	40.190029
3277.013054	353384.009859	40.195047
3279.900967	353932.079837	40.200064
3283.146462	354469.400868	40.205082
3286.956182	355005.256321	40.210100
3289.679928	355556.101728	40.215117
3293.397912	356093.635504	40.220135
3296.564057	356637.977234	40.225152
3299.849776	357159.627607	40.230170
3303.091493	357674.553181	40.235188
3306.388420	358168.169221	40.240205
3309.284316	358668.112988	40.245223
3312.199942	359174.089280	40.250240
3315.609820	359670.388049	40.255258
3318.882451	360173.657767	40.260276
3321.709049	360698.591626	40.265293
3324.925034	361219.422640	40.270311
3328.140124	361737.963857	40.275328
3331.102948	362273.036085	40.280346
3334.624685	362798.623394	40.285364
3338.165371	363344.048263	40.290381
3341.774535	363873.873234	40.295399
3344.726519	364424.606440	40.300416
3348.068288	364963.825756	40.305434
3351.501886	365508.632660	40.310452
3354.554896	366073.871406	40.315469
3357.956084	366626.562312	40.320487
3360.941473	367186.366911	40.325504
3364.412819	367765.678365	40.330522
3367.805814	368336.848767	40.335540
3371.467856	368909.187200	40.340557
3374.877557	369485.516591	40.345575
3377.973576	370071.352879	40.350592
3381.386536	370653.705420	40.355610
3384.859370	371231.625348	40.360628
3388.147920	371832.986982	40.365645
3391.829903	372418.774352	40.370663
3395.438512	373007.736813	40.375680
3399.079645	373601.658932	40.380698
3402.655122	374189.569536	40.385716
3406.344452	374782.477468	40.390733
3410.103426	375353.672633	40.395751
3413.323236	375941.335157	40.400768
3417.216147	376528.781208	40.405786
3421.058475	377108.767582	40.410804
3424.403417	377693.441620	40.415821
3427.681223	378264.240124	40.420839
3431.272517	378838.228147	40.425856
3434.600923	379420.697384	40.430874
3438.061751	379991.999933	40.435892
3441.506643	380580.674186	40.440909
3445.035210	381169.782856	40.445927
3448.641076	381760.189389	40.450944
3452.006843	382325.130317	40.455962
3455.820138	382908.560875	40.460980
3459.205818	383497.098013	40.465997
3462.632757	384063.525247	40.471015
3466.195650	384641.793695	40.476032
3469.254310	385226.677189	40.481050
3472.875369	385803.929033	40.486068
3476.319218	386386.830815	40.491085
3479.989572	386969.611397	40.496103
3483.296944	387563.270453	40.501120
3486.624310	388130.614418	40.506125
3490.364605	388649.472111	40.511130
3493.499288	389134.700823	40.516135
3496.522863	389556.219323	40.521140
3499.458317	389925.239619	40.526144
3501.622254	390241.845945	40.531149
3504.322200	390521.165350	40.536154
3505.999169	390739.086473	40.541159
3507.827883	390910.731501	40.546164
3509.491685	391054.025923	40.551168
3510.787117	391160.484436	40.556173
3512.322440	391225.917594	40.561178
3513.280724	391257.065589	40.566183
3513.939173	391268.021681	40.571188
3514.737818	391240.714547	40.576192
3515.266726	391213.856853	40.581197
3516.231605	391149.858670	40.586202
3516.435449	391085.497575	40.591207
3516.873102	390972.280661	40.596212
3517.043374	390860.351549	40.601216
3517.069159	390747.758404	40.606221
3517.342458	390618.547567	40.611226
3517.722833	390485.479883	40.616231
3517.713242	390340.039592	40.621236
3517.399869	390195.511241	40.626240
3517.291019	390033.252697	40.631245
3517.594773	389879.980279	40.636250
3517.226701	389716.744174	40.641255
3517.189628	389549.844294	40.646260
3517.114780	389374.558497	40.651264
3516.641985	389225.499857	40.656269
3516.518494	389046.304269	40.661274
3515.971615	388887.720493	40.666279
3515.928387	388730.149802	40.671284
3515.736742	388575.348122	40.676288
3515.498046	388414.857278	40.681293
3515.351842	388254.935948	40.686298
3514.815993	388097.948924	40.691303
3514.843587	387937.184997	40.696308
3514.428163	387788.925031	40.701312
3514.052239	387650.855168	40.706317
3513.651818	387491.224927	40.711322
3513.517895	387355.607717	40.716327
3513.481345	387216.948541	40.721332
3513.287242	387079.763207	40.726336
3512.789404	386953.534543	40.731341
3512.491603	386815.728874	40.736346
3512.315601	386683.930218	40.741351
3511.946729	386567.368464	40.746356
3512.070516	386447.626039	40.751360
3511.401087	386340.367466	40.756365
3511.522321	386208.087801	40.761370
3511.314464	386091.117627	40.766375
3511.224278	385995.871109	40.771380
3510.603141	385883.593860	40.776384
3510.521844	385779.928030	40.781389
3510.249522	385676.088664	40.786394
3510.062784	385580.754612	40.791399
3510.257104	385484.749748	40.796404
3509.905480	385395.697142	40.801408
3509.756306	385310.960924	40.806413
3509.546700	385211.789537	40.811418
3509.289259	385127.680345	40.816423
3509.143048	385040.349120	40.821428
3509.038998	384963.590189	40.826432
3508.459422	384888.050654	40.831437
3508.714887	384816.753054	40.836442
3508.341009	384755.116797	40.841447
3508.265986	384680.438019	40.846452
3508.236757	384605.777281	40.851456
3508.145861	384543.790768	40.856461
3508.163280	384474.793499	40.861466
3508.187759	384403.302742	40.866471
3508.292201	384338.106122	40.871476
3508.008705	384278.336689	40.876480
3507.390193	384215.110616	40.881485
3507.742978	384140.210537	40.886490
3507.264204	384092.398928	40.891495
3507.318743	384035.932596	40.896500
3507.665811	383977.894054	40.901504
3507.389761	383918.834946	40.906509
3507.056795	383865.252500	40.911514
3506.835378	383817.425286	40.916519
3506.563681	383767.546008	40.921524
3506.630881	383720.919188	40.926528
3506.369265	383677.218057	40.931533
3506.547933	383625.741501	40.936538
3506.538304	383595.835224	40.941543
3506.389854	383554.176021	40.946548
3506.480073	383504.849539	40.951552
3506.322569	383464.921022	40.956557
3506.466412	383425.199141	40.961562
3506.312939	383388.626894	40.966567
3506.056229	383350.112684	40.971572
3506.356129	383309.908240	40.976576
3506.124598	383272.992174	40.981581
3506.271707	383226.428404	40.986586
3506.017164	383207.343644	40.991591
3505.741711	383169.468010	40.996596
3505.806268	383138.201751	41.001600
3505.753678	383111.557167	41.006605
3505.752123	383066.262865	41.011610
3505.721605	383039.614741	41.016615
3505.829893	383004.552091	41.021620
3505.540456	382968.306114	41.026624
3505.591979	382938.491376	41.031629
3505.995802	382909.282155	41.036634
3505.852751	382880.896895	41.041639
3505.510077	382837.614517	41.046644
3505.507401	382809.791951	41.051648
3505.635238	382776.023038	41.056653
3505.480026	382747.766762	41.061658
3505.055547	382733.795064	41.066663
3505.252359	382704.669276	41.071668
3505.268777	382682.616711	41.076672
3505.099556	382664.230291	41.081677
3505.335810	382635.912045	41.086682
3505.341505	382602.976119	41.091687
3505.036364	382589.265258	41.096692
3505.460537	382554.457441	41.101696
3505.338221	382540.081852	41.106701
3505.267059	382510.031848	41.111706
3505.464953	382484.313653	41.116711
3505.551156	382458.104450	41.121716
3505.380979	382427.917440	41.126720
3504.967556	382411.705823	41.131725
3505.310476	382372.561743	41.136730
3505.194686	382355.870700	41.141735
3504.821410	382333.091130	41.146740
3505.059869	382316.572961	41.151744
3505.099573	382301.510423	41.156749
3505.263779	382286.453630	41.161754
3505.154162	382254.730958	41.166759
3505.168592	382230.643843	41.171764
3505.321830	382213.910208	41.176768
3504.819246	382189.574177	41.181773
3505.288392	382158.548340	41.186778
3505.017212	382142.593881	41.191783
3504.880139	382111.460379	41.196788
3504.889076	382090.019035	41.201792
3504.957814	382075.129847	41.206797
3504.831506	382043.460503	41.211802
3504.463164	382033.396301	41.216807
3504.665732	382011.949735	41.221812
3504.857703	381997.727717	41.226816
3504.582294	381991.336553	41.231821
3504.856098	381962.274322	41.236826
3504.576191	381952.603041	41.241831
3504.298627	381928.027808	41.246836
3504.412079	381912.266774	41.251840
3504.364472	381891.953298	41.256845
3504.577842	381888.841971	41.261850
3504.277632	381868.924475	41.266855
3504.390982	381863.412844	41.271860
3504.845872	381844.520439	41.276864
3504.472372	381833.439688	41.281869
3504.921485	381810.682394	41.286874
3504.447307	381808.925960	41.291879
3504.545463	381781.010403	41.296884
3504.400121	381774.395177	41.301888
3504.651613	381756.425033	41.306893
3504.870699	381739.604481	41.311898
3504.484006	381741.572845	41.316903
3504.561931	381715.288140	41.321908
3504.310833	381701.085189	41.326912
3504.224422	381695.401650	41.331917
3504.364458	381683.527552	41.336922
3504.224391	381668.289720	41.341927
3504.106009	381650.479729	41.346932
3504.352132	381643.166773	41.351936
3504.250238	381632.551684	41.356941
3504.599723	381621.941535	41.361946
3504.556849	381601.398260	41.366951
3504.606101	381585.748972	41.371956
3504.698234	381569.482508	41.376960
3504.388541	381570.243357	41.381965
3504.485604	381537.673560	41.386970
3504.265393	381532.825005	41.391975
3504.287494	381510.363935	41.396980
3504.529515	381510.528907	41.401984
3504.328525	381496.114494	41.406989
3503.986697	381481.213679	41.411994
3504.380823	381477.412485	41.416999
3504.335469	381466.305185	41.422004
3504.679755	381449.693611	41.427008
3504.530607	381438.119483	41.432013
3504.389918	381417.515273	41.437018
3504.346024	381407.348749	41.442023
3504.395667	381380.381592	41.447028
3504.280980	381366.436716	41.452032
3504.149465	381356.538361	41.457037
3504.198333	381331.377043	41.462042
3504.099325	381342.888237	41.467047
3504.207115	381330.027235	41.472052
3504.286864	381308.548825	41.477056
3504.181585	381311.896978	41.482061
3504.431035	381302.065549	41.487066
3504.401555	381304.130063	41.492071
3504.376784	381287.703928	41.497076
3504.497273	381277.053585	41.502080
3504.482801	381253.224754	41.507085
3504.593435	381237.947119	41.512090
3504.550516	381226.305267	41.517095
3504.407728	381208.880427	41.522100
3504.419052	381183.190850	41.527104
3504.573154	381179.656470	41.532109
3504.069826	381161.500175	41.537114
3504.155480	381158.205514	41.542119
3504.239127	381149.748219	41.547124
3504.344703	381126.993962	41.552128
3504.044018	381125.464401	41.557133
3504.409057	381105.797406	41.562138
3503.929853	381100.303040	41.567143
3504.209795	381095.375362	41.572148
3504.171329	381066.260084	41.577152
3504.415191	381074.359958	41.582157
3504.228375	381057.399809	41.587162
3504.239515	381041.451125	41.592167
3504.045503	381030.977599	41.597172
3504.055736	381013.248713	41.602176
3504.189344	381007.326823	41.607181
3504.199003	380984.791112	41.612186
3504.269741	380979.489557	41.617191
3503.949396	380981.879837	41.622196
3504.154934	380966.027557	41.627200
3504.132236	380957.815932	41.632205
3504.251043	380947.191197	41.637210
3504.063338	380937.886585	41.642215
3504.164145	380922.356043	41.647220
3504.264931	380914.430089	41.652224
3503.824300	380913.583912	41.657229
3504.320399	380894.709959	41.662234
3504.273493	380884.060537	41.667239
3504.125509	380876.402803	41.672244
3503.986167	380872.685884	41.677248
3504.077414	380863.438889	41.682253
3504.262544	380854.533118	41.687258
3504.195418	380849.914610	41.692263
3504.355359	380824.913436	41.697268
3504.405198	380818.470657	41.702272
3504.189029	380801.820237	41.707277
3504.361005	380781.929262	41.712282
3504.211748	380775.568818	41.717287
3504.052727	380766.335930	41.722292
3504.328340	380757.873635	41.727296
3504.138071	380738.574008	41.732301
3504.393884	380741.814260	41.737306
3503.939615	380720.623411	41.742311
3504.118674	380706.402956	41.747316
3504.053856	380703.335512	41.752320
3504.045990	380680.853260	41.757325
3504.111378	380676.086614	41.762330
3504.116959	380672.346766	41.767335
3503.684339	380652.424135	41.772340
3504.065470	380642.444553	41.777344
3504.219105	380642.140264	41.782349
3504.413247	380626.518548	41.787354
3504.309565	380626.814476	41.792359
3504.164482	380595.833611	41.797364
3504.536489	380588.322518	41.802368
3504.027197	380580.467507	41.807373
3504.407953	380559.068262	41.812378
3504.102630	380552.579851	41.817383
3503.478145	380542.606616	41.822388
3504.089288	380538.694722	41.827392
3504.031640	380534.227279	41.832397
3504.023298	380516.882606	41.837402
3504.134644	380515.669389	41.842407
3504.092633	380515.268860	41.847412
3504.538636	380484.601401	41.852416
3504.055605	380484.906433	41.857421
3504.234693	380461.809524	41.862426
3504.408641	380447.131975	41.867431
3504.180189	380438.367791	41.872436
3504.225860	380416.156693	41.877440
3503.882187	380413.514815	41.882445
3504.164096	380401.821363	41.887450
3503.773460	380400.305993	41.892455
3503.955344	380390.637616	41.897460
3504.025200	380391.719992	41.902464
3503.747160	380379.224872	41.907469
3503.850437	380369.416313	41.912474
3504.089380	380374.872001	41.917479
3503.784554	380362.584581	41.922484
3503.879861	380350.971480	41.927488
3504.120547	380334.859046	41.932493
3504.338613	380328.415025	41.937498
3503.790999	380322.473553	41.942503
3503.776341	380312.174949	41.947508
3503.917318	380308.337359	41.952512
3503.675857	380306.035389	41.957517
3503.872197	380287.081359	41.962522
3504.069710	380283.387432	41.967527
3503.931382	380276.872574	41.972532
3503.615446	380267.537204	41.977536
3503.250539	380257.955234	41.982541
3503.957130	380247.593460	41.987546
3503.930927	380269.928282	41.992551
3503.794898	380250.467233	41.997556
3504.077333	380233.559709	42.002560
3503.889104	380238.930343	42.007565
3504.005903	380239.547493	42.012570
3504.146833	380218.745518	42.017575
3504.034484	380197.474894	42.022580
3503.858484	380192.517444	42.027584
3503.692323	380189.059038	42.032589
3503.992901	380181.253952	42.037594
3504.132410	380184.054828	42.042599
3504.158547	380167.467564	42.047604
3504.123398	380150.991718	42.052608
3503.813449	380150.252033	42.057613
3503.746143	380132.026322	42.062618
3503.759823	380117.908097	42.067623
3503.694146	380119.927528	42.072628
3503.787367	380125.355420	42.077632
3503.958750	380120.241309	42.082637
3504.236716	380091.177007	42.087642
3504.140649	380094.447508	42.092647
3503.772436	380086.086848	42.097652
3504.114031	380057.775481	42.102656
3503.824388	380066.646625	42.107661
3504.215971	380064.804111	42.112666
3504.120887	380041.979201	42.117671
3504.111539	380035.621950	42.122676
3504.075244	380028.455071	42.127680
3503.949239	380006.423482	42.132685
3504.144086	379992.886987	42.137690
3503.996568	379995.250005	42.142695
3503.765912	379980.992318	42.147700
3504.057441	379964.184975	42.152704
3503.661444	379972.055592	42.157709
3503.973733	379944.613533	42.162714
3503.914465	379950.803143	42.167719
3503.949710	379944.387960	42.172724
3504.350946	379927.919334	42.177728
3504.117941	379923.530411	42.182733
3504.070121	379902.910710	42.187738
3503.932067	379888.409444	42.192743
3503.846735	379883.615660	42.197748
3504.163487	379869.602037	42.202752
3504.141968	379862.127582	42.207757
3504.104187	379845.855495	42.212762
3503.925581	379858.727722	42.217767
3503.951684	379842.191194	42.222772
3503.796912	379826.522578	42.227776
3503.436256	379835.735644	42.232781
3503.692382	379829.667036	42.237786
3503.810015	379813.879049	42.242791
3504.079510	379802.696061	42.247796
3504.002177	379790.830310	42.252800
3503.903375	379788.149677	42.257805
3503.840389	379772.212188	42.262810
3503.580272	379763.478291	42.267815
3503.524153	379766.157518	42.272820
3504.200660	379765.414485	42.277824
3504.001806	379754.076616	42.282829
3503.895553	379736.187521	42.287834
3504.028718	379738.506182	42.292839
3503.916539	379726.442446	42.297844
3504.117121	379705.478161	42.302848
3503.975553	379703.872520	42.307853
3503.770171	379695.486033	42.312858
3503.905967	379681.831595	42.317863
3503.706832	379676.597960	42.322868
3503.941921	379676.535129	42.327872
3503.580188	379665.299286	42.332877
3503.722998	379644.801918	42.337882
3503.904957	379643.221432	42.342887
3504.104622	379638.789511	42.347892
3504.122535	379630.876396	42.352896
3503.846568	379623.442120	42.357901
3504.126891	379612.257366	42.362906
3503.507709	379611.286780	42.367911
3503.469562	379598.092193	42.372916
3503.443238	379585.913103	42.377920
3503.623488	379592.599026	42.382925
3503.976434	379588.727856	42.387930
3503.985919	379590.430221	42.392935
3503.714025	379571.778773	42.397940
3503.867293	379568.244379	42.402944
3503.695657	379563.616805	42.407949
3503.790745	379552.334146	42.412954
3503.583544	379547.966535	42.417959
3503.608241	379542.392285	42.422964
3503.737351	379536.343711	42.427968
3503.940880	379544.984404	42.432973
3503.858300	379529.711204	42.437978
3503.760404	379516.195389	42.442983
3503.805706	379514.102381	42.447988
3503.671060	379513.996263	42.452992
3503.687811	379511.627990	42.457997
3503.580568	379492.085707	42.463002
3503.569451	379509.229976	42.468007
3503.620459	379492.180674	42.473012
3503.549906	379496.540868	42.478016
3503.667302	379510.765305	42.483021
3503.997752	379495.553970	42.488026
3503.755448	379469.292926	42.493031
3503.654423	379468.087816	42.498036
3503.917266	379464.459787	42.503040
3503.710232	379456.683935	42.508045
3503.810364	379439.652279	42.513050
3503.776858	379444.032057	42.518055
3504.067226	379435.923224	42.523060
3504.016230	379420.746727	42.528064
3503.604204	379410.002014	42.533069
3503.443140	379400.082394	42.538074
3503.703840	379401.592447	42.543079
3503.601046	379404.329946	42.548084
3503.472733	379387.690464	42.553088
3503.363973	379384.324648	42.558093
3503.916284	379376.174394	42.563098
3503.989659	379379.494471	42.568103
3503.448431	379385.963837	42.573108
3503.932728	379384.335545	42.578112
3503.614610	379371.999043	42.583117
3504.054597	379351.073024	42.588122
3503.855904	379354.003728	42.593127
3503.933894	379340.866998	42.598132
3503.648697	379334.171724	42.603136
3503.595780	379323.166741	42.608141
3503.740500	379316.810452	42.613146
3503.878162	379322.409472	42.618151
3503.611889	379309.123679	42.623156
3503.944450	379291.343049	42.628160
3503.826956	379295.532645	42.633165
3503.736354	379301.879918	42.638170
3503.454858	379294.624495	42.643175
3503.629378	379275.291905	42.648180
3503.584852	379274.917195	42.653184
3503.408697	379271.460286	42.658189
3503.651755	379273.202044	42.663194
3503.540942	379277.365151	42.668199
3503.542551	379278.382044	42.673204
3503.701464	379252.413510	42.678208
3503.581001	379251.007990	42.683213
3503.466545	379244.285709	42.688218
3503.443472	379257.464195	42.693223
3503.563893	379250.068922	42.698228
3503.571225	379255.663120	42.703232
3503.800088	379258.093854	42.708237
3503.974776	379229.045237	42.713242
3503.306970	379234.873342	42.718247
3503.233689	379232.010595	42.723252
3503.452996	379226.837921	42.728256
3503.470269	379236.296597	42.733261
3503.640211	379232.734102	42.738266
3503.536361	379217.515013	42.743271
3503.905112	379201.051216	42.748276
3503.828020	379200.808826	42.753280
3503.456490	379209.464199	42.758285
3503.634947	379195.523067	42.763290
3503.682499	379190.021458	42.768295
3503.195820	379181.348681	42.773300
3503.793130	379181.355760	42.778304
3503.705113	379177.477957	42.783309
3503.841939	379183.712993	42.788314
3503.872227	379172.821987	42.793319
3503.813359	379159.477920	42.798324
3503.813959	379149.405506	42.803329
3503.437114	379148.447466	42.808333
3503.664573	379145.435431	42.813338
3503.721658	379135.582996	42.818343
3503.521817	379125.109876	42.823348
3503.824776	379123.790021	42.828353
3503.500830	379117.762135	42.833357
3503.699689	379120.858920	42.838362
3503.719937	379125.179366	42.843367
3503.731121	379100.963637	42.848372
3503.903696	379094.043347	42.853377
3503.506688	379100.922349	42.858381
3503.707857	379098.626636	42.863386
3503.603059	379079.795929	42.868391
3503.505242	379080.040072	42.873396
3503.848142	379073.092852	42.878401
3503.850625	379082.248688	42.883405
3503.608357	379071.705956	42.888410
3503.798116	379059.568847	42.893415
3503.709922	379041.447666	42.898420
3504.051475	379034.017394	42.903425
3503.688541	379058.669827	42.908429
3503.882217	379029.872407	42.913434
3503.793298	379016.634780	42.918439
3503.534717	379016.929773	42.923444
3504.086626	379015.697732	42.928449
3503.915526	379003.948303	42.933453
3504.061706	378985.917219	42.938458
3504.036239	378985.056234	42.943463
3503.773596	378971.947795	42.948468
3503.775770	378953.812288	42.953473
3503.534757	378958.402966	42.958477
3503.699365	378949.042180	42.963482
3503.867061	378948.252396	42.968487
3503.900848	378933.952521	42.973492
3503.867640	378932.202544	42.978497
3503.529571	378922.336220	42.983501
3503.818258	378930.022502	42.988506
3503.762812	378918.432807	42.993511
3503.354156	378903.846780	42.998516
3503.696440	378896.568974	43.003521
3503.738755	378888.906199	43.008525
3503.902461	378883.437053	43.013530
3503.728462	378865.354791	43.018535
3503.421412	378858.332238	43.023540
3503.673869	378849.618844	43.028545
3503.777377	378856.495068	43.033549
3503.730073	378855.281446	43.038554
3503.562979	378851.975676	43.043559
3503.923750	378832.460816	43.048564
3504.090220	378827.220139	43.053569
3503.683242	378839.111413	43.058573
3503.726805	378818.832780	43.063578
3504.205931	378805.479847	43.068583
3503.960920	378794.047257	43.073588
3503.921448	378792.323699	43.078593
3503.744058	378773.071929	43.083597
3503.624141	378765.790863	43.088602
3503.659243	378758.332681	43.093607
3503.789268	378765.408207	43.098612
3503.890199	378745.273076	43.103617
3503.436675	378738.731485	43.108621
3503.917337	378731.253730	43.113626
3503.844721	378731.799109	43.118631
3503.775797	378730.538031	43.123636
3503.700445	378709.362486	43.128641
3503.580368	378707.371884	43.133645
3503.876878	378700.050409	43.138650
3503.824611	378705.094541	43.143655
3503.630312	378686.226925	43.148660
3503.939808	378670.586190	43.153665
3503.381032	378668.944721	43.158669
3503.741386	378668.989261	43.163674
3503.738866	378663.012231	43.168679
3503.622620	378651.432069	43.173684
3503.629571	378640.570039	43.178689
3503.319996	378638.634825	43.183693
3504.040693	378631.500628	43.188698
3503.555499	378648.338695	43.193703
3503.222985	378633.842270	43.198708
3503.734303	378615.244594	43.203713
3503.657555	378603.124040	43.208717
3503.330282	378602.768587	43.213722
3503.932717	378606.997054	43.218727
3503.615714	378611.269132	43.223732
3503.644673	378599.869479	43.228737
3503.567982	378592.708722	43.233741
3503.725241	378574.294173	43.238746
3503.629111	378583.338540	43.243751
3503.871532	378586.046957	43.248756
3503.764615	378574.210948	43.253761
3503.420605	378560.097837	43.258765
3503.948744	378548.822734	43.263770
3503.843411	378552.883312	43.268775
3503.817964	378548.207071	43.273780
3503.783447	378528.881725	43.278785
3503.559082	378525.915636	43.283789
3503.573004	378513.322892	43.288794
3503.595994	378522.323006	43.293799
3503.579220	378531.634624	43.298804
3503.617668	378517.842560	43.303809
3503.516260	378503.970861	43.308813
3503.671844	378496.925977	43.313818
3503.660231	378500.310435	43.318823
3503.822593	378493.722308	43.323828
3503.806257	378489.120925	43.328833
3503.672496	378475.686726	43.333837
3503.812088	378465.744774	43.338842
3503.748442	378461.532392	43.343847
3503.628198	378462.950095	43.348852
3503.680141	378452.055465	43.353857
3503.500575	378437.992619	43.358861
3503.225905	378434.907300	43.363866
3503.479088	378430.772003	43.368871
3503.664483	378441.018214	43.373876
3503.834696	378433.258825	43.378881
3503.528169	378444.371287	43.383885
3503.983851	378416.066133	43.388890
3503.755167	378417.119455	43.393895
3503.591481	378411.803741	43.398900
3503.688190	378412.576707	43.403905
3503.583803	378401.325252	43.408909
3503.873610	378375.767842	43.413914
3503.559965	378374.952401	43.418919
3503.677597	378378.723398	43.423924
3503.716969	378383.091772	43.428929
3503.588818	378376.931079	43.433933
3503.855664	378355.879292	43.438938
3503.619426	378348.820019	43.443943
3503.610160	378346.125133	43.448948
3503.769534	378350.372800	43.453953
3503.751485	378342.058148	43.458957
3503.934676	378314.635357	43.463962
3503.776600	378316.593183	43.468967
3503.703534	378310.881603	43.473972
3504.133953	378297.510763	43.478977
3503.919258	378289.354363	43.483981
3503.847739	378268.050800	43.488986
3503.935552	378272.208048	43.493991
3503.482017	378254.958184	43.498996
3503.733170	378240.649130	43.504001
3503.984423	378239.439161	43.509005
3503.839003	378235.468599	43.514010
3503.737400	378226.938215	43.519015
3503.652142	378214.462795	43.524020
3503.910906	378203.764318	43.529025
3503.615782	378219.682289	43.534029
3503.752945	378209.003037	43.539034
3503.532386	378194.590491	43.544039
3503.664138	378176.968280	43.549044
3503.866260	378173.858437	43.554049
3503.672901	378182.587608	43.559053
3503.521995	378163.585705	43.564058
3503.462238	378151.589503	43.569063
3503.517184	378139.931256	43.574068
3503.677933	378135.785106	43.579073
3503.177999	378136.474353	43.584077
3503.607136	378145.232300	43.589082
3503.301001	378145.026112	43.594087
3503.113065	378145.538859	43.599092
3503.345544	378150.690659	43.604097
3503.304546	378160.743815	43.609101
3503.682663	378143.336994	43.614106
3503.347010	378136.751233	43.619111
3503.536947	378128.759750	43.624116
3503.876763	378115.759265	43.629121
3503.492283	378119.431618	43.634125
3503.452550	378123.151211	43.639130
3503.617044	378119.640348	43.644135
3503.619101	378127.550147	43.649140
3503.892024	378116.849408	43.654145
3503.532874	378102.331562	43.659149
3503.731571	378098.103103	43.664154
3503.616487	378113.153291	43.669159
3503.635940	378100.381494	43.674164
3503.772437	378079.986048	43.679169
3503.398083	378080.935231	43.684173
3503.602126	378079.961638	43.689178
3503.539126	378079.818754	43.694183
3503.720831	378072.311830	43.699188
3503.623255	378061.466166	43.704193
3503.524369	378049.450682	43.709197
3503.721781	378035.811367	43.714202
3503.567851	378031.486035	43.719207
3503.573626	378041.964227	43.724212
3503.635061	378038.138991	43.729217
3503.390062	378034.260456	43.734221
3503.157876	378010.336883	43.739226
3503.908938	378003.248645	43.744231
3503.638506	378001.943093	43.749236
3503.810011	378011.784647	43.754241
3503.466362	378008.481281	43.759245
3504.062000	377993.354620	43.764250
3503.762757	377997.216991	43.769255
3503.509216	377986.090738	43.774260
3503.317005	377982.356465	43.779265
3503.254415	377992.947219	43.784269
3503.287226	377983.912263	43.789274
3503.115039	377992.739871	43.794279
3503.262112	377982.186168	43.799284
3503.416357	377986.002284	43.804289
3503.380135	377997.021270	43.809293
3503.384404	377979.495430	43.814298
3503.648823	377960.860173	43.819303
3503.578951	377955.987402	43.824308
3503.829933	377948.876469	43.829313
3503.378263	377960.978555	43.834317
3503.118176	377959.773108	43.839322
3503.533213	377960.241406	43.844327
3503.305820	377959.971898	43.849332
3503.368836	377956.273580	43.854337
3503.157472	377948.752467	43.859341
3503.328187	377930.767892	43.864346
3503.672248	377927.737332	43.869351
3503.833123	377931.603277	43.874356
3503.960573	377921.128965	43.879361
3503.679650	377928.778315	43.884365
3503.754904	377913.479536	43.889370
3503.398113	377906.744465	43.894375
3503.464830	377896.178007	43.899380
3503.599139	377892.977121	43.904385
3503.745781	377901.372815	43.909389
3503.695075	377894.589355	43.914394
3503.728218	377879.373526	43.919399
3503.372290	377866.915350	43.924404
3503.551780	377872.228175	43.929409
3503.533366	377873.299140	43.934413
3503.552860	377862.358607	43.939418
3503.424403	377873.697433	43.944423
3503.389664	377871.744167	43.949428
3503.826875	377849.342539	43.954433
3503.745756	377848.261408	43.959437
3503.716345	377840.126495	43.964442
3503.985205	377829.273709	43.969447
3503.277656	377822.136237	43.974452
3503.674805	377803.022085	43.979457
3503.658281	377802.490321	43.984461
3503.560773	377794.696824	43.989466
3503.773371	377804.735416	43.994471
3503.366845	377816.576055	43.999476
3503.978210	377804.117555	44.004481
3503.394522	377788.490495	44.009485
3503.469678	377779.016396	44.014490
3503.659753	377773.339445	44.019495
3503.395507	377774.016873	44.024500
3503.894797	377768.596264	44.029505
3503.522066	377774.657724	44.034509
3503.759496	377753.381349	44.039514
3503.450667	377749.055038	44.044519
3503.497532	377740.806304	44.049524
3503.757428	377736.593568	44.054529
3503.375715	377753.110430	44.059533
3503.675911	377744.618165	44.064538
3503.663465	377718.980937	44.069543
3503.726230	377712.510168	44.074548
3503.853320	377697.533772	44.079553
3503.332303	377706.823557	44.084557
3503.294235	377704.234923	44.089562
3503.412908	377712.736821	44.094567
3503.464500	377714.992191	44.099572
3503.560961	377692.796956	44.104577
3503.612099	377686.277150	44.109581
3503.529785	377684.484009	44.114586
3503.599286	377679.792656	44.119591
3503.838459	377688.682478	44.124596
3503.773699	377684.266705	44.129601
3503.579259	377670.027888	44.134605
3503.545737	377648.565371	44.139610
3503.760231	377646.267467	44.144615
3503.515314	377655.513616	44.149620
3503.716176	377651.157590	44.154625
3503.461140	377655.547152	44.159629
3503.800956	377622.986580	44.164634
3503.476243	377630.108763	44.169639
3503.342515	377623.567301	44.174644
3503.557937	377631.850437	44.179649
3503.541880	377634.396298	44.184653
3503.480996	377637.356213	44.189658
3503.469195	377632.194432	44.194663
3503.576405	377605.698841	44.199668
3503.834873	377591.032299	44.204673
3503.591574	377593.410602	44.209677
3503.378998	377597.818893	44.214682
3503.545884	377598.886008	44.219687
3503.744657	377592.648074	44.224692
3503.695104	377568.975153	44.229697
3503.388406	377571.516094	44.234701
3503.464925	377556.191541	44.239706
3503.436068	377566.777076	44.244711
3503.536095	377576.401117	44.249716
3503.618083	377563.517518	44.254721
3503.409302	377568.484796	44.259725
3503.562355	377541.931044	44.264730
3503.407723	377534.884160	44.269735
3503.448444	377535.945786	44.274740
3503.695289	377533.210356	44.279745
3503.293666	377537.623104	44.284749
3503.437370	377524.602559	44.289754
3503.541274	377535.294292	44.294759
3503.521160	377536.416407	44.299764
3503.955886	377514.625437	44.304769
3503.826117	377509.024448	44.309773
3503.330454	377508.288634	44.314778
3503.382583	377506.575974	44.319783
3503.694566	377515.556067	44.324788
3503.856995	377508.866025	44.329793
3503.649591	377485.879335	44.334797
3503.753214	377479.961654	44.339802
3503.853328	377479.360575	44.344807
3503.759899	377471.693548	44.349812
3503.436497	377450.963514	44.354817
3503.593901	377446.207365	44.359821
3503.882364	377439.090416	44.364826
3503.692030	377445.758982	44.369831
3503.384143	377443.162114	44.374836
3503.472397	377439.078223	44.379841
3503.238403	377420.419763	44.384845
3503.377318	377402.668898	44.389850
3503.295091	377400.112660	44.394855
3503.061149	377406.610076	44.399860
3503.303407	377405.147148	44.404865
3502.903282	377403.505980	44.409869
3503.183741	377407.251328	44.414874
3502.907380	377412.407358	44.419879
3503.015776	377417.553434	44.424884
3503.369836	377410.095445	44.429889
3503.169668	377421.572915	44.434893
3503.308657	377408.756562	44.439898
3503.224147	377415.967988	44.444903
3503.151959	377420.913690	44.449908
3503.583408	377420.489152	44.454913
3503.324312	377420.936851	44.459917
3503.189089	377419.813390	44.464922
3503.469943	377431.163942	44.469927
3503.449479	377422.722301	44.474932
3503.502398	377426.122084	44.479937
3503.372708	377434.281769	44.484941
3503.829211	377430.597505	44.489946
3504.165919	377406.532761	44.494951
3503.390182	377407.443670	44.499956
3503.667699	377394.198442	44.504961
3503.504407	377399.641827	44.509965
3503.482430	377400.433576	44.514970
3503.367242	377384.096400	44.519975
3503.648615	377375.734211	44.524980
3503.596771	377376.352632	44.529985
3503.259914	377370.962411	44.534989
3503.427957	377363.966228	44.539994
3503.506884	377372.754275	44.544999
3503.277354	377370.043272	44.550004
3503.655448	377363.395418	44.555009
3503.617143	377368.106849	44.560013
3503.320115	377349.687242	44.565018
3503.384205	377338.052750	44.570023
3503.455084	377334.429439	44.575028
3503.959724	377334.781837	44.580033
3503.342451	377345.435016	44.585037
3503.703391	377344.589217	44.590042
3503.815740	377342.485494	44.595047
3503.417381	377321.131348	44.600052
3503.651510	377303.594308	44.605057
3503.486237	377305.731371	44.610061
3503.730738	377302.131481	44.615066
3503.539320	377302.873711	44.620071
3503.683012	377298.704735	44.625076
3503.966599	377271.214480	44.630081
3503.517828	377283.341749	44.635085
3503.670805	377274.567428	44.640090
3503.636842	377273.962107	44.645095
3503.521832	377261.770884	44.650100
3503.328602	377248.854384	44.655105
3503.020836	377242.289501	44.660109
3503.340225	377242.569443	44.665114
3503.211673	377243.327171	44.670119
3502.972549	377243.797150	44.675124
3503.148757	377239.572156	44.680129
3502.829947	377252.263912	44.685133
3503.224697	377239.305329	44.690138
3503.105602	377247.183584	44.695143
3502.903579	377246.960931	44.700148
3503.172685	377271.692609	44.705153
3503.066323	377284.884920	44.710157
3503.350460	377283.059266	44.715162
3503.451029	377271.673346	44.720167
3503.105157	377257.229398	44.725172
3503.564259	377253.392092	44.730177
3503.394254	377258.912865	44.735181
3503.363250	377259.502557	44.740186
3503.250580	377265.217752	44.745191
3503.528426	377262.197609	44.750196
3503.622519	377266.303099	44.755201
3503.493934	377276.573812	44.760205
3503.269341	377269.537940	44.765210
3503.378687	377274.505833	44.770215
3503.319044	377259.813151	44.775220
3503.724759	377236.551341	44.780225
3502.954476	377239.928663	44.785229
3503.332127	377241.522055	44.790234
3503.438518	377244.659043	44.795239
3503.292223	377248.955151	44.800244
3503.616049	377238.729409	44.805249
3503.229697	377253.441270	44.810253
3503.407312	377244.561305	44.815258
3503.304499	377251.114324	44.820263
3503.205524	377253.113730	44.825268
3503.464881	377243.406897	44.830273
3503.503534	377254.541430	44.835277
3503.076855	377233.827608	44.840282
3503.105022	377227.413102	44.845287
3503.354798	377221.497713	44.850292
3503.402730	377226.144656	44.855297
3503.491686	377221.628223	44.860301
3503.786910	377221.301526	44.865306
3503.753581	377220.365438	44.870311
3503.422883	377218.891337	44.875316
3503.609751	377221.227094	44.880321
3503.491455	377219.693978	44.885325
3503.904801	377199.381494	44.890330
3503.713840	377201.955032	44.895335
3503.419026	377199.737619	44.900340
3503.604219	377207.135369	44.905345
3503.636231	377204.357572	44.910349
3503.392121	377186.514547	44.915354
3503.484483	377180.624037	44.920359
3503.420088	377173.130414	44.925364
3503.312193	377167.195253	44.930369
3503.264387	377176.206865	44.935373
3503.603792	377168.242432	44.940378
3503.572986	377172.316804	44.945383
3503.601942	377167.860722	44.950388
3503.650631	377161.264910	44.955393
3503.486327	377146.792218	44.960397
3503.485899	377135.752892	44.965402
3503.374401	377140.323305	44.970407
3503.151015	377141.553873	44.975412
3503.651340	377128.883795	44.980417
3503.413906	377137.518419	44.985421
3503.629810	377133.083652	44.990426
3503.335416	377127.076224	44.995431
3503.299954	377116.754635	45.000436
3503.682531	377106.468700	45.005441
3503.357816	377120.534968	45.010445
3503.374248	377115.495836	45.015450
3503.577532	377113.148803	45.020455
3503.149834	377109.121008	45.025460
3503.845511	377104.559520	45.030465
3503.466936	377106.857493	45.035469
3503.528116	377107.203692	45.040474
3503.487948	377085.716486	45.045479
3503.591930	377077.992740	45.050484
3503.353534	377076.097067	45.055489
3503.319527	377077.450313	45.060493
3503.830964	377074.444101	45.065498
3503.778375	377083.761721	45.070503
3503.274278	377061.737382	45.075508
3503.647051	377043.593285	45.080513
3503.264241	377040.321465	45.085517
3503.273470	377043.041417	45.090522
3503.196624	377043.689232	45.095527
3503.562329	377039.408824	45.100532
3503.512591	377038.729685	45.105537
3503.497270	377037.638130	45.110541
3503.693740	377038.675147	45.115546
3504.057871	377029.841957	45.120551
3503.232341	377015.346569	45.125556
3503.589986	377010.660457	45.130561
3503.348958	377015.276797	45.135565
3503.370237	377016.773922	45.140570
3503.600432	377015.923349	45.145575
3503.216836	377010.057185	45.150580
3503.410498	377012.824291	45.155585
3503.479096	377015.178756	45.160589
3503.567692	376987.235849	45.165594
3503.440589	376981.380004	45.170599
3503.480968	376987.376275	45.175604
3503.580571	376982.502029	45.180609
3503.284139	376987.152567	45.185613
3503.393065	376976.986168	45.190618
3503.642466	376982.364368	45.195623
3503.629978	376968.147407	45.200628
3503.792796	376957.082224	45.205633
3503.388730	376950.685132	45.210637
3503.436735	376950.804491	45.215642
3503.884946	376940.126598	45.220647
3503.498396	376957.661993	45.225652
3503.581615	376941.649374	45.230657
3503.470915	376927.346180	45.235661
3503.638965	376919.078119	45.240666
3503.767132	376924.551801	45.245671
3503.409751	376916.188751	45.250676
3503.685277	376914.160953	45.255681
3503.540959	376909.783108	45.260685
3503.464920	376889.649576	45.265690
3503.369037	376880.024250	45.270695
3503.395881	376884.445642	45.275700
3503.576415	376881.237367	45.280705
3503.518009	376881.704217	45.285709
3503.743089	376881.032502	45.290714
3503.550700	376879.460215	45.295719
3503.302698	376860.574782	45.300724
3503.549363	376844.231053	45.305729
3503.299986	376849.510070	45.310733
3503.472124	376843.250794	45.315738
3503.587566	376851.600771	45.320743
3503.158599	376854.542625	45.325748
3503.480409	376847.369427	45.330753
3503.377613	376850.743004	45.335757
3503.313736	376846.250690	45.340762
3503.663872	376850.417490	45.345767
3503.303728	376841.825936	45.350772
3503.559104	376819.223552	45.355777
3503.208978	376815.641313	45.360781
3503.181853	376816.662812	45.365786
3503.550002	376806.786058	45.370791
3503.162502	376818.191571	45.375796
3503.186169	376815.440503	45.380801
3503.375401	376824.287541	45.385805
3503.569287	376815.989938	45.390810
3503.524571	376823.474977	45.395815
3502.989191	376833.708368	45.400820
3503.153015	376821.116826	45.405825
3503.161852	376828.847759	45.410829
3503.122898	376830.125487	45.415834
3503.309369	376825.491850	45.420839
3503.432368	376835.010695	45.425844
3503.715554	376827.055082	45.430849
3503.483401	376822.640240	45.435853
3503.307234	376799.012314	45.440858
3503.399914	376780.022114	45.445863
3503.222227	376795.922088	45.450868
3503.625076	376792.144503	45.455873
3503.474065	376790.336746	45.460877
3503.391194	376793.173020	45.465882
3503.569737	376798.028289	45.470887
3503.624044	376787.336319	45.475892
3503.413948	376760.228991	45.480897
3503.389476	376766.693397	45.485901
3503.582996	376761.473608	45.490906
3503.418697	376765.289328	45.495911
3503.135811	376772.761156	45.500916
3504.009449	376760.388051	45.505921
3503.822202	376766.165978	45.510925
3503.511840	376742.711851	45.515930
3503.968780	376732.057959	45.520935
3503.965226	376723.231955	45.525940
3503.666759	376728.442440	45.530945
3503.632902	376720.104512	45.535949
3503.992760	376706.388189	45.540954
3504.149157	376700.004199	45.545959
3503.669111	376703.997021	45.550964
3503.560608	376670.590846	45.555969
3503.348502	376667.978785	45.560973
3503.608596	376667.250659	45.565978
3503.612485	376668.597929	45.570983
3503.280062	376675.416266	45.575988
3503.549630	376669.166997	45.580993
3503.165683	376679.605413	45.585997
3503.524620	376672.960474	45.591002
3503.520542	376659.250797	45.596007
3503.272686	376654.024461	45.601012
3503.473775	376644.275823	45.606017
3503.236179	376642.430875	45.611021
3503.398645	376647.670247	45.616026
3503.485294	376638.448422	45.621031
3503.792292	376635.423624	45.626036
3503.915531	376630.698216	45.631041
3503.640149	376626.798910	45.636045
3503.300362	376611.336319	45.641050
3503.662783	376604.461892	45.646055
3503.379291	376612.849549	45.651060
3503.706529	376603.131830	45.656065
3503.561195	376611.650263	45.661069
3503.272692	376603.657802	45.666074
3503.292550	376599.737256	45.671079
3503.090270	376591.069820	45.676084
3503.463268	376574.477083	45.681089
3503.368938	376577.009949	45.686093
3503.437335	376576.515616	45.691098
3503.293253	376568.627498	45.696103
3503.109369	376584.452226	45.701108
3503.636253	376580.120853	45.706113
3503.369888	376572.023140	45.711117
3503.668954	376579.123207	45.716122
3503.694280	376577.643671	45.721127
3503.506481	376567.854747	45.726132
3503.513726	376538.881503	45.731137
3503.372906	376553.809166	45.736141
3503.222611	376542.717060	45.741146
3503.430160	376546.524889	45.746151
3502.985097	376547.358102	45.751156
3503.332586	376551.118372	45.756161
3503.348736	376552.183908	45.761165
3503.520602	376546.967515	45.766170
3503.577013	376554.538362	45.771175
3503.286381	376549.140722	45.776180
3503.611647	376540.517058	45.781185
3503.245559	376534.622620	45.786189
3503.346833	376525.322148	45.791194
3503.514255	376519.267057	45.796199
3503.394018	376516.258919	45.801204
3503.577222	376521.622210	45.806209
3503.534185	376523.409319	45.811213
3503.323789	376525.146577	45.816218
3503.252406	376525.717227	45.821223
3503.353978	376536.155235	45.826228
3503.917374	376516.251100	45.831233
3503.497110	376501.589712	45.836237
3503.522122	376486.705309	45.841242
3503.666059	376483.426479	45.846247
3503.550621	376486.395104	45.851252
3503.739216	376489.900700	45.856257
3503.442981	376479.111446	45.861261
3503.535822	376461.138520	45.866266
3503.702213	376448.444710	45.871271
3503.582823	376455.509206	45.876276
3503.781287	376454.154912	45.881281
3503.857480	376460.145600	45.886285
3503.376748	376442.466831	45.891290
3503.591042	376424.067708	45.896295
3503.308050	376426.019937	45.901300
3503.578202	376416.362071	45.906305
3503.371104	376421.303787	45.911309
3503.542365	376417.003180	45.916314
3503.421154	376421.778701	45.921319
3503.307990	376420.041253	45.926324
3503.521841	376413.037663	45.931329
3503.594744	376398.145656	45.936333
3503.330126	376387.402252	45.941338
3503.318962	376381.273627	45.946343
3503.386805	376387.926990	45.951348
3503.330781	376385.417418	45.956353
3503.355485	376381.725011	45.961357
3503.286775	376377.614954	45.966362
3503.509742	376379.512636	45.971367
3503.390191	376388.713821	45.976372
3503.659732	376384.397674	45.981377
3503.461951	376362.604325	45.986381
3503.231723	376353.381656	45.991386
3503.185072	376364.428176	45.996391
3503.574017	376356.481188	46.001396
3503.848982	376356.564669	46.006401
3503.226427	376355.034928	46.011405
3503.330459	376350.388833	46.016410
3503.528655	376352.595668	46.021415
3503.049138	376354.528096	46.026420
3503.655706	376348.072884	46.031425
3503.313052	376336.324348	46.036429
3503.452717	376331.316508	46.041434
3503.366907	376329.142313	46.046439
3503.124263	376327.374458	46.051444
3503.189470	376331.713537	46.056449
3502.967468	376339.048639	46.061453
3503.319943	376325.791208	46.066458
3503.445598	376333.809006	46.071463
3503.222622	376339.465461	46.076468
3503.420931	376338.976024	46.081473
3503.485449	376334.895774	46.086477
3503.266338	376337.219453	46.091482
3503.768753	376332.739304	46.096487
3503.569540	376339.612948	46.101492
3503.797842	376315.132269	46.106497
3503.398565	376300.849036	46.111501
3503.627875	376290.612559	46.116506
3503.758231	376294.661543	46.121511
3503.609637	376302.442901	46.126516
3503.720963	376288.638544	46.131521
3503.036738	376284.651219	46.136525
3503.051759	376275.440635	46.141530
3503.150744	376267.717522	46.146535
3502.981374	376272.907657	46.151540
3503.223876	376266.026694	46.156545
3502.937528	376279.374972	46.161549
3503.206636	376290.854886	46.166554
3503.585755	376288.963300	46.171559
3503.436461	376287.078940	46.176564
3503.374685	376272.462541	46.181569
3503.230033	376271.747521	46.186573
3503.670993	376271.423215	46.191578
3503.782647	376277.942488	46.196583
3503.676118	376271.828923	46.201588
3503.682229	376255.929966	46.206593
3503.172388	376252.703599	46.211597
3503.260219	376240.429125	46.216602
3503.742588	376234.146148	46.221607
3503.145282	376246.093718	46.226612
3503.433025	376236.280409	46.231617
3503.371701	376240.537755	46.236621
3503.414635	376242.031485	46.241626
3503.390341	376252.642083	46.246631
3503.325390	376249.777803	46.251636
3503.524354	376241.988008	46.256641
3503.042808	376236.900307	46.261645
3502.859300	376247.739567	46.266650
3503.280548	376241.949545	46.271655
3503.074076	376248.468242	46.276660
3503.467758	376239.019733	46.281665
3503.431764	376254.108991	46.286669
3503.059489	376227.306742	46.291674
3503.184105	376226.803518	46.296679
3503.014500	376226.041569	46.301684
3503.115835	376221.065211	46.306689
3503.017018	376253.740978	46.311693
3503.527039	376253.507499	46.316698
3503.240674	376234.704146	46.321703
3502.963998	376236.553640	46.326708
3503.144064	376233.421697	46.331713
3503.279482	376244.312285	46.336717
3503.317287	376239.066173	46.341722
3503.316447	376233.698987	46.346727
3503.087902	376237.067057	46.351732
3503.341796	376230.591270	46.356737
3503.519301	376239.542037	46.361741
3503.105470	376230.907967	46.366746
3503.185013	376236.236811	46.371751
3503.008793	376242.343744	46.376756
3503.626863	376234.233328	46.381761
3503.154933	376244.227909	46.386765
3503.535761	376246.685679	46.391770
3503.548476	376245.386180	46.396775
3503.197166	376251.800591	46.401780
3503.435617	376242.224004	46.406785
3503.599699	376247.539482	46.411789
3503.570130	376234.596782	46.416794
3503.546871	376206.416650	46.421799
3503.569050	376204.657797	46.426804
3503.762537	376202.642934	46.431809
3503.660902	376203.625354	46.436813
3503.435960	376202.795843	46.441818
3503.527526	376196.218531	46.446823
3503.349923	376179.814421	46.451828
3503.490025	376170.991022	46.456833
3503.513231	376173.352713	46.461837
3503.050866	376173.272957	46.466842
3503.293039	376178.245425	46.471847
3503.103009	376181.302174	46.476852
3503.226761	376177.059924	46.481857
3503.177155	376183.121413	46.486861
3503.189786	376185.103229	46.491866
3503.354001	376180.752837	46.496871
3503.269020	376176.060293	46.501876
3503.376321	376174.033617	46.506881
3503.091718	376178.428014	46.511885
3502.815885	376181.523764	46.516890
3503.055572	376174.490611	46.521895
3503.122199	376177.939206	46.526900
3503.287247	376179.896927	46.531905
3502.999575	376185.156647	46.536909
3503.058212	376184.307742	46.541914
3503.256361	376195.417355	46.546919
3503.323220	376195.991592	46.551924
3503.295096	376187.169355	46.556929
3503.057689	376190.716885	46.561933
3503.066670	376190.028449	46.566938
3503.335247	376194.742376	46.571943
3503.258568	376191.981692	46.576948
3503.192912	376193.339972	46.581953
3503.245816	376189.821145	46.586957
3503.418783	376184.197548	46.591962
3503.641176	376190.750202	46.596967
3503.045664	376197.457592	46.601972
3503.428358	376180.685106	46.606977
3503.331981	376169.915046	46.611981
3503.389479	376160.697720	46.616986
3503.618213	376162.060335	46.621991
3503.153479	376156.105126	46.626996
3503.395693	376162.909016	46.632001
3503.083236	376167.867419	46.637005
3503.362740	376162.964634	46.642010
3503.530972	376161.360745	46.647015
3503.407290	376170.511760	46.652020
3503.635902	376166.380115	46.657025
3503.442425	376165.825431	46.662029
3503.310279	376159.410660	46.667034
3503.448919	376146.492214	46.672039
3503.369153	376138.314042	46.677044
3503.074905	376133.349337	46.682049
3502.857474	376145.745614	46.687053
3502.981381	376140.638495	46.692058
3503.052875	376140.499779	46.697063
3503.118629	376142.117087	46.702068
3503.209094	376145.409298	46.707073
3503.494365	376146.279681	46.712077
3502.920296	376145.734290	46.717082
3503.205803	376152.556774	46.722087
3503.236297	376150.186129	46.727092
3503.250312	376155.118359	46.732097
3503.258074	376155.015154	46.737101
3503.235690	376153.899255	46.742106
3503.553900	376147.133486	46.747111
3503.139184	376158.136504	46.752116
3503.395123	376158.655414	46.757121
3503.304389	376145.646045	46.762125
3503.125989	376160.732415	46.767130
3503.540014	376150.746503	46.772135
3503.322529	376157.546757	46.777140
3503.709680	376148.531679	46.782145
3503.542776	376160.080559	46.787149
3503.235592	376137.490416	46.792154
3503.447871	376122.143853	46.797159
3503.326838	376121.603152	46.802164
3503.705396	376121.822876	46.807169
3503.773289	376118.937586	46.812173
3503.388186	376121.033154	46.817178
3503.670808	376115.824633	46.822183
3503.359327	376118.671657	46.827188
3503.652644	376097.258385	46.832193
3503.397144	376094.780329	46.837197
3503.665969	376083.977949	46.842202
3503.705081	376077.383473	46.847207
3503.670897	376087.207145	46.852212
3503.654427	376079.654868	46.857217
3503.681115	376069.170565	46.862221
3503.562787	376051.281714	46.867226
3503.363466	376043.809209	46.872231
3503.271500	376046.545227	46.877236
3503.640802	376045.647207	46.882241
3503.371766	376051.692532	46.887245
3503.205637	376058.281192	46.892250
3503.680714	376044.749922	46.897255
3503.575541	376027.749259	46.902260
3503.644438	376017.665256	46.907265
3503.413917	376013.300939	46.912269
3503.643706	376020.005072	46.917274
3503.633184	376015.427920	46.922279
3503.580071	376019.862048	46.927284
3503.720014	376003.076991	46.932289
3503.390910	375983.415433	46.937293
3503.511467	375985.278450	46.942298
3503.771493	375975.189657	46.947303
3503.419094	375979.467610	46.952308
3503.563401	375981.937351	46.957313
3503.288225	375983.405070	46.962317
3503.393714	375974.027495	46.967322
3503.230099	375952.203085	46.972327
3503.128296	375956.594044	46.977332
3503.771491	375938.177769	46.982337
3503.260388	375943.803519	46.987341
3503.356844	375951.266403	46.992346
3503.837205	375940.455980	46.997351
3503.193381	375941.498684	47.002356
3503.265251	375942.682611	47.007361
3503.351471	375951.775056	47.012365
3503.390720	375944.341128	47.017370
3503.325676	375952.974191	47.022375
3502.926556	375953.596660	47.027380
3503.549817	375940.143676	47.032385
3503.391500	375946.883739	47.037389
3503.041424	375924.300257	47.042394
3503.220341	375917.861709	47.047399
3503.061225	375921.396887	47.052404
3503.121410	375914.417503	47.057409
3503.050116	375926.841617	47.062413
3503.294476	375940.487658	47.067418
3503.118475	375923.549021	47.072423
3502.991862	375935.880132	47.077428
3503.129718	375945.600331	47.082433
3503.141396	375957.858699	47.087437
3503.203432	375953.753366	47.092442
3503.390421	375961.583485	47.097447
3503.261159	375948.274905	47.102452
3503.461824	375924.027287	47.107457
3503.146807	375924.661898	47.112461
3503.356427	375920.914780	47.117466
3503.176508	375917.483609	47.122471
3503.082603	375937.669467	47.127476
3503.107911	375926.752923	47.132481
3503.076231	375922.687838	47.137485
3502.880216	375923.456256	47.142490
3503.229843	375919.559821	47.147495
3502.974275	375930.435995	47.152500
3503.219491	375930.168068	47.157505
3502.824694	375948.213938	47.162509
3503.268267	375957.809494	47.167514
3503.457431	375954.141923	47.172519
3502.873834	375947.213445	47.177524
3503.340884	375942.687971	47.182529
3503.185572	375941.720264	47.187533
3503.191637	375941.032284	47.192538
3503.254916	375941.352725	47.197543
3503.209888	375951.203581	47.202548
3503.636997	375939.689351	47.207553
3503.404560	375948.323441	47.212557
3503.413896	375946.464860	47.217562
3503.265462	375945.801305	47.222567
3503.133781	375952.562593	47.227572
3503.313574	375937.857011	47.232577
3503.927902	375941.727774	47.237581
3503.568013	375941.580943	47.242586
3503.599604	375920.514192	47.247591
3503.356805	375913.302903	47.252596
3503.624398	375905.629377	47.257601
3503.111636	375913.137704	47.262605
3503.276134	375915.299018	47.267610
3503.428265	375909.068197	47.272615
3503.196640	375912.055231	47.277620
3503.074070	375912.583109	47.282625
3503.183765	375914.498720	47.287629
3503.255326	375923.720672	47.292634
3503.112440	375919.698604	47.297639
3502.984352	375927.324173	47.302644
3503.295949	375914.174817	47.307649
3503.293760	375921.576991	47.312653
3503.163602	375920.350941	47.317658
3503.409486	375913.393073	47.322663
3503.502688	375912.538698	47.327668
3503.677425	375915.588675	47.332673
3503.459327	375896.189329	47.337677
3503.016217	375892.799763	47.342682
3503.292249	375886.218675	47.347687
3503.212904	375886.866903	47.352692
3503.699519	375890.554368	47.357697
3503.188006	375891.754212	47.362701
3503.167036	375894.173776	47.367706
3503.422898	375887.239764	47.372711
3503.168558	375895.622961	47.377716
3503.200503	375896.100975	47.382721
3503.300519	375895.016592	47.387725
3503.204523	375897.549764	47.392730
3503.637054	375900.533552	47.397735
3503.836274	375894.880327	47.402740
3503.619995	375880.924128	47.407745
3503.377203	375869.286852	47.412749
3503.229534	375859.262481	47.417754
3503.559281	375860.253024	47.422759
3503.381259	375857.101351	47.427764
3503.458885	375859.657951	47.432769
3503.697479	375861.222511	47.437773
3503.253355	375860.631136	47.442778
3503.468608	375859.706591	47.447783
3503.071119	375860.379677	47.452788
3503.429691	375856.812499	47.457793
3503.124758	375843.429909	47.462797
3503.128102	375831.092357	47.467802
3503.372864	375822.048843	47.472807
3503.426472	375830.714048	47.477812
3503.358598	375825.967885	47.482817
3503.701625	375826.396722	47.487821
3503.460300	375820.736821	47.492826
3503.658402	375828.132786	47.497831
3503.601182	375824.911140	47.502836
3503.714869	375808.791507	47.507841
3503.742398	375803.343469	47.512845
3503.558483	375812.275157	47.517850
3503.731405	375799.147686	47.522855
3503.412987	375809.982954	47.527860
3503.647480	375812.082335	47.532865
3503.310034	375791.811521	47.537869
3503.698383	375767.101715	47.542874
3503.651584	375765.124817	47.547879
3503.170078	375765.022648	47.552884
3503.440290	375756.534704	47.557889
3503.557099	375764.706633	47.562893
3503.544327	375763.538331	47.567898
3503.784418	375755.894561	47.572903
3503.643811	375739.586170	47.577908
3503.667511	375727.321679	47.582913
3503.508209	375731.136707	47.587917
3503.484710	375723.509164	47.592922
3503.713265	375723.879788	47.597927
3503.118373	375713.875208	47.602932
3503.399899	375701.493640	47.607937
3503.507952	375698.958086	47.612941
3503.380068	375699.334186	47.617946
3503.736855	375683.328692	47.622951
3503.245208	375692.283619	47.627956
3503.409309	375693.783651	47.632961
3503.435310	375700.113064	47.637965
3503.593584	375697.823939	47.642970
3503.598937	375690.013771	47.647975
3503.163121	375674.311632	47.652980
3503.265208	375653.055540	47.657985
3503.103035	375661.220721	47.662989
3503.220559	375660.108127	47.667994
3503.480400	375653.453251	47.672999
3503.372308	375666.112194	47.678004
3503.257421	375662.568973	47.683009
3502.885517	375666.748295	47.688013
3502.767081	375663.536313	47.693018
3502.998265	375661.184786	47.698023
3503.175249	375670.924303	47.703028
3503.249838	375664.832886	47.708033
3503.137806	375663.273284	47.713037
3503.206552	375666.034794	47.718042
3503.248257	375670.021545	47.723047
3503.313201	375664.033401	47.728052
3503.420461	375666.483581	47.733057
3503.256835	375672.435988	47.738061
3503.291022	375664.468636	47.743066
3503.257926	375666.966442	47.748071
3503.045435	375671.247746	47.753076
3503.374842	375670.228841	47.758081
3503.227865	375671.142132	47.763085
3502.985793	375674.817629	47.768090
3503.240148	375678.999692	47.773095
3503.188624	375685.443111	47.778100
3503.518253	375680.303413	47.783105
3503.386426	375686.021860	47.788109
3503.344087	375681.704069	47.793114
3503.502717	375681.398955	47.798119
3503.163477	375689.083386	47.803124
3503.230983	375677.320690	47.808129
3503.166049	375680.739252	47.813133
3503.276577	375685.808903	47.818138
3503.588965	375680.926298	47.823143
3503.287175	375658.996390	47.828148
3503.364444	375650.106501	47.833153
3503.346634	375650.261705	47.838157
3503.528495	375651.351942	47.843162
3503.504512	375646.980372	47.848167
3503.204747	375658.575836	47.853172
3503.282818	375649.100772	47.858177
3503.182273	375658.528051	47.863181
3503.029758	375660.892114	47.868186
3503.395574	375657.705326	47.873191
3503.264392	375654.876911	47.878196
3503.294178	375657.364776	47.883201
3503.175022	375660.919096	47.888205
3503.028204	375657.177428	47.893210
3503.374335	375649.745806	47.898215
3502.961248	375664.589656	47.903220
3503.126608	375657.873406	47.908225
3503.402741	375660.602131	47.913229
3503.435080	375665.531525	47.918234
3503.266868	375659.503928	47.923239
3503.425807	375663.777388	47.928244
3503.299138	375651.587519	47.933249
3503.239637	375638.573050	47.938253
3503.372316	375628.377119	47.943258
3503.516374	375624.284222	47.948263
3503.074643	375634.579422	47.953268
3503.450002	375628.287831	47.958273
3503.432828	375634.420586	47.963277
3503.367104	375626.418148	47.968282
3503.207716	375637.304632	47.973287
3503.256520	375637.474742	47.978292
3503.525939	375627.664183	47.983297
3503.331153	375635.402098	47.988301
3503.064733	375641.269013	47.993306
3503.358007	375631.276625	47.998311
3503.034189	375642.723275	48.003316
3503.335157	375636.214515	48.008321
3503.148498	375634.793893	48.013325
3503.446259	375636.298234	48.018330
3503.162142	375624.184121	48.023335
3502.976107	375611.723820	48.028340
3502.997749	375617.087336	48.033345
3502.954501	375636.858346	48.038349
3503.155787	375647.001016	48.043354
3503.641927	375648.882565	48.048359
3503.255853	375642.355234	48.053364
3503.418398	375626.024311	48.058369
3503.362799	375612.144364	48.063373
3503.211026	375603.290673	48.068378
3503.282899	375603.838689	48.073383
3503.076873	375614.096631	48.078388
3503.425110	375605.367390	48.083393
3503.583751	375612.617011	48.088397
3503.422925	375614.956955	48.093402
3503.475503	375606.884937	48.098407
3503.474561	375621.231222	48.103412
3503.636193	375610.700031	48.108417
3503.927456	375603.124453	48.113421
3503.659018	375589.964941	48.118426
3503.678097	375579.023851	48.123431
3503.400110	375586.011823	48.128436
3503.845140	375575.105142	48.133441
3503.447340	375561.737139	48.138445
3503.241094	375543.938272	48.143450
3503.877506	375538.953553	48.148455
3503.577416	375542.205806	48.153460
3503.623987	375539.451030	48.158465
3503.500358	375538.427431	48.163469
3503.336347	375534.866528	48.168474
3503.592924	375512.339533	48.173479
3503.348651	375506.730928	48.178484
3503.638449	375492.541969	48.183489
3503.387272	375501.179116	48.188493
3503.193304	375495.689741	48.193498
3503.305858	375502.107250	48.198503
3503.192677	375503.549377	48.203508
3503.303870	375505.719139	48.208513
3503.383024	375502.806589	48.213517
3503.582648	375512.313632	48.218522
3503.625567	375506.888558	48.223527
3503.422159	375491.098733	48.228532
3503.757141	375475.325538	48.233537
3503.775359	375466.317758	48.238541
3503.524524	375466.865918	48.243546
3503.617236	375470.539382	48.248551
3503.324872	375477.860326	48.253556
3503.521753	375460.608179	48.258561
3503.610293	375446.629079	48.263565
3503.484880	375436.321279	48.268570
3503.638257	375430.726111	48.273575
3503.356724	375443.717785	48.278580
3503.114292	375427.120123	48.283585
3503.178747	375444.584875	48.288589
3503.276658	375447.952276	48.293594
3503.257981	375441.850134	48.298599
3503.296851	375443.191914	48.303604
3503.298554	375442.173936	48.308609
3503.335812	375445.957916	48.313613
3503.238620	375438.316533	48.318618
3503.432782	375440.956484	48.323623
3503.039660	375438.169464	48.328628
3503.316612	375430.825049	48.333633
3503.167998	375407.090203	48.338637
3503.085238	375411.020345	48.343642
3503.237174	375400.668691	48.348647
3503.299134	375411.189563	48.353652
3503.384658	375400.517727	48.358657
3503.217152	375409.192540	48.363661
3503.309951	375412.102887	48.368666
3503.497849	375405.306721	48.373671
3503.164113	375405.282938	48.378676
3503.643389	375410.625009	48.383681
3503.610413	375409.154647	48.388685
3503.324517	375412.353794	48.393690
3503.508235	375418.200453	48.398695
3503.174273	375407.162506	48.403700
3503.532868	375402.298001	48.408705
3503.334500	375390.857059	48.413709
3503.167383	375379.385737	48.418714
3503.519993	375375.387032	48.423719
3503.426412	375378.047039	48.428724
3503.074386	375371.666903	48.433729
3503.461916	375366.492575	48.438733
3503.335215	375370.124424	48.443738
3503.411686	375376.954649	48.448743
3503.255520	375373.494239	48.453748
3503.019322	375372.056003	48.458753
3503.276669	375380.536473	48.463757
3503.242890	375382.805472	48.468762
3503.412418	375378.606776	48.473767
3503.317917	375382.030038	48.478772
3503.411502	375378.072281	48.483777
3503.309749	375379.232798	48.488781
3503.334846	375373.683339	48.493786
3503.597005	375363.517746	48.498791
3503.199603	375353.965159	48.503796
3503.114094	375335.562062	48.508801
3503.783046	375348.149137	48.513805
3503.329891	375351.145797	48.518810
3503.585334	375348.001870	48.523815
3503.385943	375353.883667	48.528820
3503.419275	375344.059487	48.533825
3503.548704	375346.989485	48.538829
3503.392249	375338.289098	48.543834
3503.572158	375327.195330	48.548839
3503.377653	375322.520001	48.553844
3503.674441	375319.191477	48.558849
3503.425423	375319.510418	48.563853
3503.400967	375316.487049	48.568858
3503.860204	375315.600233	48.573863
3503.364178	375307.843816	48.578868
3503.354240	375287.241168	48.583873
3503.305684	375280.355177	48.588877
3502.916289	375284.537302	48.593882
3503.121130	375277.306007	48.598887
3503.237374	375278.762747	48.603892
3503.313394	375273.027164	48.608897
3503.425021	375275.171433	48.613901
3503.084974	375280.922854	48.618906
3503.572142	375280.616674	48.623911
3503.141533	375285.415803	48.628916
3503.174177	375282.943019	48.633921
3503.425237	375286.438844	48.638925
3503.519426	375281.565250	48.643930
3503.225940	375283.646376	48.648935
3503.309242	375293.375357	48.653940
3503.264689	375288.625444	48.658945
3503.119651	375297.958092	48.663949
3503.070330	375297.278857	48.668954
3503.420015	375292.034192	48.673959
3503.165165	375299.298363	48.678964
3503.115161	375292.081921	48.683969
3503.293415	375298.005773	48.688973
3503.342810	375293.495379	48.693978
3503.411247	375297.986681	48.698983
3503.196287	375302.853465	48.703988
3503.532239	375286.240621	48.708993
3503.323763	375264.880800	48.713997
3503.111539	375262.446725	48.719002
3503.189228	375252.920756	48.724007
3503.154073	375257.275817	48.729012
3503.327188	375258.367448	48.734017
3503.364131	375268.307259	48.739021
3503.536147	375259.707550	48.744026
3503.712637	375252.531607	48.749031
3503.273972	375262.597482	48.754036
3503.452302	375257.049219	48.759041
3503.538787	375260.062323	48.764045
3503.331766	375262.994642	48.769050
3503.462137	375229.167956	48.774055
3503.197909	375226.665788	48.779060
3503.477178	375218.964850	48.784065
3503.642099	375223.008477	48.789069
3503.441472	375220.038387	48.794074
3503.635685	375216.293640	48.799079
3503.421578	375229.961524	48.804084
3503.616361	375222.197632	48.809089
3503.530808	375208.907335	48.814093
3503.206871	375204.761196	48.819098
3503.387695	375180.923264	48.824103
3503.418150	375189.337895	48.829108
3503.472687	375185.869597	48.834113
3503.180914	375191.664273	48.839117
3503.013347	375186.552239	48.844122
3503.269928	375188.622724	48.849127
3502.980476	375193.424986	48.854132
3503.287949	375191.570113	48.859137
3503.234725	375185.447957	48.864141
3503.393363	375196.487779	48.869146
3503.621757	375192.686752	48.874151
3503.396493	375196.130701	48.879156
3503.351014	375202.878486	48.884161
3503.271561	375198.642822	48.889165
3503.291479	375186.429639	48.894170
3503.449292	375164.019813	48.899175
3503.306564	375171.113659	48.904180
3503.463437	375159.591056	48.909185
3503.440539	375154.837704	48.914189
3503.565650	375155.479059	48.919194
3503.388481	375151.665831	48.924199
3503.327486	375153.532151	48.929204
3503.532607	375159.757021	48.934209
3503.302349	375162.565834	48.939213
3503.385120	375162.374457	48.944218
3503.360962	375137.449673	48.949223
3503.418370	375129.631169	48.954228
3503.191033	375118.550850	48.959233
3503.511034	375119.797324	48.964237
3503.472097	375124.203871	48.969242
3503.343323	375125.928284	48.974247
3503.475137	375128.400052	48.979252
3503.645175	375122.166280	48.984257
3503.635648	375128.068968	48.989261
3503.362106	375113.180383	48.994266
3503.456660	375092.611992	48.999271
3503.430908	375098.491812	49.004276
3503.167281	375092.555526	49.009281
3503.550577	375088.119510	49.014285
3503.383138	375090.384217	49.019290
3503.379719	375087.662750	49.024295
3503.293630	375084.649107	49.029300
3503.632529	375084.391802	49.034305
3503.589230	375091.622566	49.039309
3503.503651	375086.573870	49.044314
3503.534772	375059.910573	49.049319
3503.586964	375058.731980	49.054324
3503.480278	375050.964839	49.059329
3503.431108	375053.210851	49.064333
3503.370694	375058.612851	49.069338
3503.542359	375063.164171	49.074343
3503.260718	375064.963627	49.079348
3503.477313	375049.387043	49.084353
3503.095534	375033.828736	49.089357
3503.038787	375038.721414	49.094362
3503.559193	375043.573726	49.099367
3503.237540	375029.659329	49.104372
3503.038537	375012.240641	49.109377
3503.225032	375018.926347	49.114381
3503.058773	375031.391185	49.119386
3503.279264	375022.529391	49.124391
3503.227367	375027.014309	49.129396
3503.163873	375013.109969	49.134401
3503.139898	375026.391743	49.139405
3503.106341	375027.694113	49.144410
3503.449115	375019.041922	49.149415
3503.380345	375020.070049	49.154420
3503.308754	375015.909434	49.159425
3503.277246	375026.724991	49.164429
3503.461541	375020.972256	49.169434
3503.097572	375017.544667	49.174439
3503.340670	375024.272298	49.179444
3503.429455	375020.645949	49.184449
3503.290570	375028.858449	49.189453
3503.398817	375027.289435	49.194458
3503.670225	375019.513391	49.199463
3503.401114	375020.624064	49.204468
3503.254025	374998.364096	49.209473
3503.636801	374988.408277	49.214477
3503.460371	374996.092537	49.219482
3503.707085	374980.307667	49.224487
3503.659179	374998.935049	49.229492
3503.803018	374985.710165	49.234497
3503.566589	374967.585133	49.239501
3503.184186	374963.066653	49.244506
3503.516111	374945.614878	49.249511
3503.298250	374954.246874	49.254516
3503.502433	374948.643608	49.259521
3503.699883	374953.241739	49.264525
3503.449934	374943.614870	49.269530
3503.862956	374937.673341	49.274535
3503.600031	374934.458706	49.279540
3503.465093	374917.131599	49.284545
3503.508379	374911.782700	49.289549
3503.340960	374922.848705	49.294554
3503.762468	374915.405033	49.299559
3503.466527	374915.527897	49.304564
3503.357845	374903.843705	49.309569
3503.591699	374884.830298	49.314573
3503.218011	374879.725373	49.319578
3503.234571	374875.754307	49.324583
3503.039581	374884.433577	49.329588
3503.301618	374884.544543	49.334593
3503.240106	374880.255135	49.339597
3503.269301	374890.577823	49.344602
3503.344838	374888.098234	49.349607
3503.288062	374895.560099	49.354612
3503.499045	374882.807875	49.359617
3503.544148	374883.538194	49.364621
3503.610255	374884.621314	49.369626
3503.680630	374881.760982	49.374631
3503.374975	374866.317763	49.379636
3503.569015	374850.846417	49.384641
3503.292361	374848.244441	49.389645
3503.001287	374844.779877	49.394650
3503.126091	374846.515088	49.399655
3503.010681	374857.013269	49.404660
3502.752945	374849.091907	49.409665
3502.935537	374856.643125	49.414669
3502.836798	374855.132264	49.419674
3503.394012	374873.613167	49.424679
3503.395091	374886.789276	49.429684
3503.633723	374868.105791	49.434689
3503.453149	374859.358239	49.439693
3503.209669	374851.917933	49.444698
3503.465823	374855.896299	49.449703
3503.436414	374854.069231	49.454708
3503.137306	374848.265705	49.459713
3503.464661	374850.986388	49.464717
3503.198885	374851.460606	49.469722
3503.411595	374846.186664	49.474727
3503.056625	374854.992979	49.479732
3502.990730	374857.343396	49.484737
3503.033045	374843.371396	49.489741
3503.047500	374853.314864	49.494746
3503.261741	374851.398403	49.499751
3503.163375	374864.463054	49.504756
3503.623467	374855.970343	49.509761
3503.457566	374850.858004	49.514765
3503.349692	374860.032252	49.519770
3503.533253	374838.355858	49.524775
3502.997523	374835.871150	49.529780
3503.181609	374815.924398	49.534785
3503.508229	374812.820053	49.539789
3503.083195	374821.790076	49.544794
3503.454978	374811.454392	49.549799
3503.232986	374816.881966	49.554804
3503.011231	374811.854764	49.559809
3503.139515	374810.842196	49.564813
3503.097183	374821.023585	49.569818
3503.478733	374816.079069	49.574823
3503.210827	374819.148231	49.579828
3503.248482	374820.439349	49.584833
3503.403999	374819.804037	49.589837
3503.156053	374822.284984	49.594842
3503.750333	374818.044521	49.599847
3503.666047	374817.345369	49.604852
3503.602876	374811.784349	49.609857
3503.764538	374801.838003	49.614861
3503.630162	374801.324830	49.619866
3503.622057	374783.621493	49.624871
3502.990719	374799.186969	49.629876
3502.964416	374798.961959	49.634881
3503.416756	374791.487953	49.639885
3503.213729	374798.464210	49.644890
3503.408673	374798.026162	49.649895
3503.071599	374799.274772	49.654900
3503.122797	374797.078836	49.659905
3503.413076	374799.194887	49.664909
3503.085147	374803.621718	49.669914
3503.431631	374786.193011	49.674919
3502.872726	374800.526043	49.679924
3503.232795	374797.212910	49.684929
3503.859220	374803.574731	49.689933
3503.135169	374786.111763	49.694938
3503.214289	374767.478886	49.699943
3503.019267	374766.110430	49.704948
3503.458219	374767.567046	49.709953
3503.595164	374766.680295	49.714957
3503.203381	374768.802425	49.719962
3503.741647	374766.783861	49.724967
3503.213161	374770.988027	49.729972
3503.251235	374774.797378	49.734977
3503.412303	374760.704828	49.739981
3503.231501	374766.812706	49.744986
3503.567935	374772.813377	49.749991
3503.203697	374772.947039	49.754996
3503.292365	374769.498747	49.760001
3503.426693	374749.865077	49.765005
3503.017423	374745.045572	49.770010
3503.409544	374731.654168	49.775015
3503.079244	374733.995516	49.780020
3503.080379	374730.052312	49.785025
3503.249548	374737.122363	49.790029
3503.421104	374736.789762	49.795034
3503.339200	374739.422527	49.800039
3503.150180	374743.471281	49.805044
3503.350534	374731.051376	49.810049
3503.445027	374741.490966	49.815053
3503.200564	374750.050898	49.820058
3503.585532	374738.034245	49.825063
3503.165821	374742.094031	49.830068
3503.335113	374735.097196	49.835073
3503.116949	374737.878689	49.840077
3503.403356	374735.136819	49.845082
3503.282423	374728.134989	49.850087
3503.523130	374746.055489	49.855092
3503.589531	374719.564453	49.860097
3503.673043	374698.692361	49.865101
3503.226062	374703.061710	49.870106
3503.529294	374700.062803	49.875111
3503.449381	374691.477365	49.880116
3503.771115	374692.621828	49.885121
3503.525855	374691.032375	49.890125
3503.262819	374689.878168	49.895130
3503.477993	374672.037736	49.900135
3503.295313	374664.587783	49.905140
3503.366330	374669.587495	49.910145
3503.518011	374663.407430	49.915149
3503.381674	374658.926328	49.920154
3503.466316	374660.947709	49.925159
3503.396501	374657.880586	49.930164
3503.459152	374660.414191	49.935169
3503.472378	374663.388046	49.940173
3503.309627	374661.073301	49.945178
3503.543633	374654.447784	49.950183
3503.127686	374642.710342	49.955188
3503.039863	374624.027478	49.960193
3503.132810	374630.499100	49.965197
3503.075254	374630.940403	49.970202
3503.201882	374621.711799	49.975207
3503.132380	374632.050155	49.980212
3503.110752	374623.480925	49.985217
3503.548370	374621.910702	49.990221
3503.510142	374627.767125	49.995226
3503.339575	374616.474196	50.000231
3503.008164	374633.747503	50.005236
3503.521433	374621.023722	50.010241
3503.750731	374622.793300	50.015245
3503.483658	374629.016586	50.020250
3503.620673	374621.083650	50.025255
3503.521185	374622.599955	50.030260
3503.540296	374602.144993	50.035265
3503.351114	374598.867799	50.040269
3503.241671	374589.600196	50.045274
3503.534609	374580.116354	50.050279
3503.120759	374591.068782	50.055284
3503.164858	374592.689576	50.060289
3503.410148	374587.893761	50.065293
3502.947702	374593.613753	50.070298
3503.255300	374596.617388	50.075303
3503.306898	374594.446815	50.080308
3503.408459	374587.867663	50.085313
3503.089655	374602.442619	50.090317
3503.363595	374600.923708	50.095322
3503.165715	374595.053268	50.100327
3503.003781	374599.072317	50.105332
3503.085837	374601.857233	50.110337
3503.504473	374592.455273	50.115341
3503.370127	374595.681399	50.120346
3503.491748	374594.669879	50.125351
3503.244494	374601.780348	50.130356
3503.440274	374584.935005	50.135361
3503.601627	374567.255660	50.140365
3503.428897	374558.608554	50.145370
3503.481405	374551.274025	50.150375
3503.596857	374560.870911	50.155380
3503.480919	374554.504199	50.160385
3503.898048	374556.218648	50.165389
3503.339406	374542.392424	50.170394
3503.498280	374524.052078	50.175399
3503.742794	374514.753939	50.180404
3503.797056	374512.964503	50.185409
3503.604586	374517.191887	50.190413
3503.449043	374519.098620	50.195418
3503.767564	374484.732823	50.200423
3503.434271	374482.775716	50.205428
3503.295136	374484.425481	50.210433
3503.669432	374477.854070	50.215437
3503.691557	374473.653148	50.220442
3503.483575	374472.363043	50.225447
3503.582258	374480.868784	50.230452
3503.596567	374455.072626	50.235457
3503.563278	374440.196689	50.240461
3503.320490	374440.540090	50.245466
3503.760103	374433.424157	50.250471
3503.536603	374440.505461	50.255476
3503.566755	374449.378168	50.260481
3503.628998	374418.461462	50.265485
3503.618351	374405.871314	50.270490
3503.546575	374398.836220	50.275495
3503.516149	374409.906144	50.280500
3503.969239	374399.404877	50.285505
3503.745348	374395.090213	50.290509
3503.270253	374379.597284	50.295514
3503.329897	374370.913403	50.300519
3503.000222	374374.831803	50.305524
3503.194716	374368.136173	50.310529
3503.264587	374372.347537	50.315533
3503.186119	374377.345478	50.320538
3503.438102	374373.133645	50.325543
3503.296922	374377.251185	50.330548
3503.423990	374376.187924	50.335553
3503.608768	374367.179009	50.340557
3503.309462	374373.661806	50.345562
3503.485881	374364.069147	50.350567
3503.250469	374368.379647	50.355572
3503.207284	374372.914135	50.360577
3503.355332	374373.501001	50.365581
3503.011150	374354.604165	50.370586
3503.202671	374342.948668	50.375591
3503.050954	374352.308024	50.380596
3503.444808	374351.431525	50.385601
3502.950212	374338.358236	50.390605
3502.783493	374355.936313	50.395610
3503.395330	374370.516854	50.400615
3503.282284	374381.218284	50.405620
3503.299331	374363.892353	50.410625
3503.239987	374349.376629	50.415629
3503.409306	374334.137935	50.420634
3503.225153	374337.753520	50.425639
3503.332712	374343.536061	50.430644
3503.043813	374331.727569	50.435649
3503.384770	374335.921519	50.440653
3503.103976	374338.331376	50.445658
3503.490785	374334.250850	50.450663
3503.309999	374337.179087	50.455668
3503.375099	374339.788638	50.460673
3503.397526	374341.438306	50.465677
3503.240310	374350.925720	50.470682
3503.238379	374344.057638	50.475687
3502.893074	374352.099404	50.480692
3502.946812	374348.580287	50.485697
3503.288543	374341.505250	50.490701
3502.860535	374349.305715	50.495706
3503.238084	374338.434811	50.500711
3503.226548	374352.427090	50.505716
3503.021828	374339.257101	50.510721
3503.217058	374351.003621	50.515725
3503.186379	374346.683845	50.520730
3503.413989	374330.189491	50.525735
3503.345578	374323.102976	50.530740
3503.179665	374282.047183	50.535745
3503.088588	374245.583738	50.540749
3502.704126	374201.916896	50.545754
3502.521773	374141.607215	50.550759
3502.611453	374084.892043	50.555764
3502.395903	374005.483638	50.560769
3502.106933	373928.172591	50.565773
3501.850815	373840.833664	50.570778
3501.913236	373731.414898	50.575783
3501.070623	373642.514799	50.580788
3500.907110	373541.678431	50.585793
3500.938917	373422.495451	50.590797
3500.692272	373305.035074	50.595802
3500.172548	373178.637803	50.600807
3499.638627	373047.256464	50.605812
3499.235803	372915.345214	50.610817
3498.825962	372768.832910	50.615821
3497.995462	372626.914678	50.620826
3497.733123	372480.250849	50.625831
3497.184254	372349.454764	50.630836
3496.592740	372201.264788	50.635841
3496.543834	372040.981289	50.640845
3495.761028	371885.493999	50.645850
3495.381396	371720.987792	50.650855
3494.905428	371559.243619	50.655860
3494.215152	371389.748245	50.660865
3494.328342	371218.547920	50.665869
3493.348385	371048.893460	50.670874
3493.084135	370864.141174	50.675879
3492.611827	370686.773091	50.680884
3491.988338	370499.379391	50.685889
3491.553620	370314.270070	50.690893
3490.234273	370132.759665	50.695898
3490.221626	369940.891238	50.700903
3489.780399	369759.978198	50.705908
3488.898937	369568.576188	50.710913
3488.365296	369381.341482	50.715917
3487.560043	369181.097810	50.720922
3487.352262	368992.817716	50.725927
3486.335048	368795.175295	50.730932
3486.121705	368601.450017	50.735937
3485.519235	368400.560101	50.740941
3484.448809	368205.976360	50.745946
3484.153989	368004.501717	50.750951
3483.629300	367805.632084	50.755956
3483.247605	367605.212445	50.760961
3482.298030	367395.977054	50.765965
3481.633536	367200.154359	50.770970
3481.480398	366976.416400	50.775975
3480.733209	366779.739891	50.780980
3480.081543	366567.018796	50.785985
3479.489865	366352.353581	50.790989
3478.510127	366144.083865	50.795994
3478.294328	365932.664731	50.800999
3477.333573	365708.895438	50.806004
3476.735546	365498.196199	50.811009
3476.494856	365277.822034	50.816013
3475.466156	365068.715456	50.821018
3474.840735	364842.140993	50.826023
3474.452600	364633.872534	50.831028
3473.253278	364411.457590	50.836033
3473.161602	364199.959845	50.841037
3472.510898	363989.007491	50.846042
3471.489968	363755.569471	50.851047
3470.724363	363545.269338	50.856052
3470.100781	363320.366341	50.861057
3469.772721	363106.254750	50.866061
3468.884437	362892.001743	50.871066
3468.512157	362667.946395	50.876071
3467.526084	362459.330071	50.881076
3466.706648	362238.549365	50.886081
3466.147693	362019.202230	50.891085
3465.453284	361809.569991	50.896090
3464.898566	361575.614741	50.901095
3463.883684	361376.005684	50.906100
3463.212023	361151.481516	50.911105
3462.738050	360932.064991	50.916109
3462.461650	360726.127766	50.921114
3461.680775	360499.327686	50.926119
3460.834726	360282.358879	50.931124
3460.110721	360060.229734	50.936129
3459.387549	359841.890873	50.941133
3458.548159	359625.579635	50.946138
3458.027300	359407.232262	50.951143
3457.189622	359202.216957	50.956148
3456.367890	358990.709431	50.961153
3456.195476	358769.148737	50.966157
3454.972346	358559.763968	50.971162
3454.732697	358344.217375	50.976167
3454.147748	358127.146724	50.981172
3453.315017	357910.266970	50.986177
3452.433882	357706.193788	50.991181
3451.815109	357486.784529	50.996186
3451.618906	357272.905887	51.001191
3450.705451	357048.451819	51.006196
3449.992802	356836.968667	51.011201
3449.160652	356617.996465	51.016205
3448.594817	356413.002895	51.021210
3448.009201	356185.642966	51.026215
3446.954392	355977.391260	51.031220
3446.268663	355759.842694	51.036225
3445.597883	355554.964012	51.041229
3445.022541	355348.008101	51.046234
3444.456637	355133.695277	51.051239
3443.677797	354937.432736	51.056244
3443.085009	354717.829132	51.061249
3442.746022	354502.765219	51.066253
3441.705440	354293.842700	51.071258
3441.138634	354077.769629	51.076263
3440.308199	353860.083151	51.081268
3439.406551	353650.041749	51.086273
3439.448775	353444.482012	51.091277
3438.498426	353242.030523	51.096282
3437.728516	353015.907217	51.101287
3436.936021	352817.704624	51.106292
3435.982100	352603.671698	51.111297
3435.639948	352391.551698	51.116301
3434.888459	352184.840029	51.121306
3434.367662	351974.782586	51.126311
3433.582944	351761.050339	51.131316
3432.893961	351547.302094	51.136321
3432.250273	351332.400569	51.141325
3431.776309	351130.221957	51.146330
3431.196887	350918.846205	51.151335
3430.269488	350710.731409	51.156340
3429.823696	350498.671164	51.161345
3429.167123	350284.403751	51.166349
3428.263302	350075.901021	51.171354
3427.806546	349847.678690	51.176359
3427.278026	349650.007980	51.181364
3426.438249	349430.243302	51.186369
3425.633045	349220.525507	51.191373
3424.595024	349009.851124	51.196378
3424.227571	348797.670078	51.201383
3423.389768	348588.820382	51.206388
3422.936034	348377.491268	51.211393
3422.052479	348174.297504	51.216397
3421.181435	347959.724069	51.221402
3420.675685	347760.388635	51.226407
3419.715992	347559.724413	51.231412
3419.469886	347349.707538	51.236417
3418.867725	347145.778346	51.241421
3418.094319	346942.817229	51.246426
3417.734733	346731.365224	51.251431
3416.992543	346532.190104	51.256436
3415.855542	346322.183035	51.261441
3415.104051	346102.442237	51.266445
3414.511810	345908.739004	51.271450
3414.287871	345697.312634	51.276455
3413.759921	345498.252764	51.281460
3412.879932	345291.026562	51.286465
3412.113949	345076.883809	51.291469
3411.598961	344875.223539	51.296474
3410.685203	344656.775571	51.301479
3409.879928	344454.905222	51.306484
3409.283343	344250.175848	51.311489
3408.779864	344033.620601	51.316493
3408.106099	343834.883570	51.321498
3407.353624	343636.260135	51.326503
3406.749448	343434.227231	51.331508
3406.256637	343222.961729	51.336513
3405.655787	343014.639771	51.341517
3404.529698	342806.552870	51.346522
3404.398234	342590.595363	51.351527
3403.392132	342396.156948	51.356532
3403.069142	342180.406442	51.361537
3402.469073	341962.102635	51.366541
3401.384080	341767.445592	51.371546
3400.508799	341558.907477	51.376551
3399.918300	341351.341807	51.381556
3399.381621	341145.446939	51.386561
3398.606303	340942.440062	51.391565
3397.799093	340746.157660	51.396570
3397.593307	340531.884668	51.401575
3396.491064	340327.501998	51.406580
3395.854493	340132.412522	51.411585
3395.327262	339920.428319	51.416589
3394.815433	339716.001200	51.421594
3394.221293	339508.328141	51.426599
3393.396304	339304.992886	51.431604
3392.605080	339103.458986	51.436609
3392.248843	338891.495206	51.441613
3391.194613	338701.431218	51.446618
3390.787970	338487.055774	51.451623
3389.722296	338292.919453	51.456628
3389.434839	338088.960756	51.461633
3388.741472	337876.614191	51.466637
3388.002373	337678.096851	51.471642
3387.482352	337472.900187	51.476647
3386.677936	337269.988007	51.481652
3386.042480	337061.320793	51.486657
3385.361805	336851.209051	51.491661
3384.353967	336646.417880	51.496666
3383.967922	336438.065646	51.501671
3383.106571	336250.229653	51.506676
3382.807593	336051.154132	51.511681
3382.397294	335839.850879	51.516685
3381.474732	335633.846639	51.521690
3380.794094	335428.134453	51.526695
3379.967257	335229.012687	51.531700
3379.314006	335015.225018	51.536705
3378.569543	334804.760544	51.541709
3377.804480	334618.584956	51.546714
3377.011861	334406.726719	51.551719
3376.451919	334203.486572	51.556724
3375.851015	334015.043131	51.561729
3375.586625	333814.020819	51.566733
3374.620924	333612.956085	51.571738
3374.194053	333399.713125	51.576743
3373.169966	333210.239743	51.581748
3372.650294	333002.738260	51.586753
3372.131780	332791.595491	51.591757
3371.197248	332608.267157	51.596762
3370.831535	332394.400486	51.601767
3370.072397	332193.655444	51.606772
3369.123291	331997.140493	51.611777
3368.613957	331787.240746	51.616781
3367.803160	331585.382002	51.621786
3367.075743	331381.981998	51.626791
3366.412385	331195.603062	51.631796
3365.444981	330992.825466	51.636801
3365.040277	330796.475741	51.641805
3364.293346	330598.091994	51.646810
3363.781200	330395.011615	51.651815
3363.247309	330199.673619	51.656820
3362.529083	330003.193147	51.661825
3361.998539	329800.903274	51.666829
3361.745363	329599.969238	51.671834
3360.889375	329396.074895	51.676839
3359.884956	329200.299508	51.681844
3358.987872	328990.631319	51.686849
3358.694042	328781.987357	51.691853
3357.703055	328593.616952	51.696858
3357.200000	328392.566463	51.701863
3356.606458	328198.174702	51.706868
3356.101448	327999.465771	51.711873
3355.473060	327794.232695	51.716877
3354.309153	327587.479803	51.721882
3354.093125	327381.340247	51.726887
3353.040283	327193.485398	51.731892
3352.483794	327000.332308	51.736897
3352.196477	326796.977622	51.741901
3350.891431	326598.060663	51.746906
3350.707635	326392.880899	51.751911
3349.853485	326203.973862	51.756916
3349.481952	325996.531347	51.761921
3348.682493	325801.020495	51.766925
3347.536257	325599.733577	51.771930
3347.158159	325397.840924	51.776935
3346.557855	325201.176861	51.781940
3345.947048	325010.980974	51.786945
3345.167039	324809.354109	51.791949
3344.397168	324615.057832	51.796954
3343.745774	324410.761733	51.801959
3342.974843	324219.978280	51.806964
3342.531113	324031.230433	51.811969
3342.147854	323815.764050	51.816973
3341.173730	323620.963068	51.821978
3340.737925	323417.699800	51.826983
3339.914411	323217.145319	51.831988
3339.291743	323022.923899	51.836993
3338.812832	322816.305127	51.841997
3337.713717	322619.382863	51.847002
3337.128893	322422.658883	51.852007
3336.097702	322223.026061	51.857012
3335.564341	322026.471269	51.862017
3335.153007	321829.642116	51.867021
3334.360354	321642.879241	51.872026
3334.110953	321448.951705	51.877031
3333.362457	321245.070759	51.882036
3332.513468	321041.612624	51.887041
3332.340619	320841.968209	51.892045
3331.240540	320639.669187	51.897050
3330.757035	320446.998657	51.902055
3329.894633	320252.554376	51.907060
3329.272277	320053.539463	51.912065
3328.658201	319848.284584	51.917069
3327.756022	319651.757411	51.922074
3327.404728	319452.214531	51.927079
3326.615503	319259.080590	51.932084
3325.740935	319065.475958	51.937089
3325.106741	318876.874457	51.942093
3324.449243	318678.855157	51.947098
3323.543265	318478.684962	51.952103
3323.062557	318279.312806	51.957108
3322.216824	318088.680709	51.962113
3321.635377	317893.270375	51.967117
3321.032762	317707.258727	51.972122
3320.733766	317506.633999	51.977127
3319.823338	317310.103219	51.982132
3318.951714	317119.676989	51.987137
3318.317484	316922.999887	51.992141
3317.557876	316731.078330	51.997146
3317.236337	316533.128764	52.002151
3316.585912	316339.585001	52.007156
3315.788000	316154.059605	52.012161
3315.181747	315955.339093	52.017165
3314.375507	315758.508631	52.022170
3313.821165	315561.154139	52.027175
3313.134850	315365.322469	52.032180
3312.083447	315170.184749	52.037185
3312.050040	314974.783787	52.042189
3311.206960	314788.448189	52.047194
3310.462298	314592.853434	52.052199
3309.528124	314400.929571	52.057204
3308.821427	314212.712522	52.062209
3308.594879	314006.951128	52.067213
3307.764203	313837.137763	52.072218
3307.227065	313622.588840	52.077223
3306.372323	313447.049312	52.082228
3305.606066	313250.207739	52.087233
3305.171322	313062.582218	52.092237
3304.180830	312870.384374	52.097242
3303.779801	312671.370466	52.102247
3303.031445	312476.408979	52.107252
3302.355997	312290.042462	52.112257
3301.519914	312093.846430	52.117261
3300.759296	311916.226937	52.122266
3300.006348	311715.026109	52.127271
3299.573864	311529.052769	52.132276
3298.995959	311347.991261	52.137281
3298.302029	311151.872939	52.142285
3297.407425	310964.392972	52.147290
3297.183616	310774.056438	52.152295
3296.138970	310590.317390	52.157300
3295.520998	310403.225641	52.162305
3295.382198	310193.063327	52.167309
3294.296102	310012.945879	52.172314
3293.848959	309824.654806	52.177319
3293.191986	309628.018749	52.182324
3292.460947	309438.422336	52.187329
3291.631064	309251.209476	52.192333
3290.838018	309059.839736	52.197338
3290.139014	308864.558699	52.202343
3289.720750	308675.369969	52.207348
3288.794539	308480.455294	52.212353
3288.457713	308298.892565	52.217357
3287.571776	308105.957188	52.222362
3287.106439	307917.564146	52.227367
3286.392765	307726.281619	52.232372
3285.538255	307545.589089	52.237377
3285.024999	307352.975570	52.242381
3284.287803	307150.745881	52.247386
3283.876776	306969.524003	52.252391
3283.154342	306780.838881	52.257396
3282.021791	306588.143909	52.262401
3281.749045	306397.069752	52.267405
3280.944097	306213.133402	52.272410
3280.314212	306023.439389	52.277415
3279.572604	305843.057656	52.282420
3278.860585	305653.121449	52.287425
3278.306770	305463.440066	52.292429
3277.625462	305274.848135	52.297434
3277.333245	305088.104311	52.302439
3276.315453	304902.366299	52.307444
3275.870522	304709.585299	52.312449
3275.179499	304507.395190	52.317453
3274.049628	304330.281533	52.322458
3273.686846	304137.741398	52.327463
3273.062900	303956.116198	52.332468
3272.122748	303768.047002	52.337473
3271.662739	303586.802848	52.342477
3270.962927	303399.229929	52.347482
3270.379646	303211.434605	52.352487
3269.705080	303026.556595	52.357492
3268.871438	302835.846339	52.362497
3268.524099	302644.498657	52.367501
3267.771948	302459.428477	52.372506
3267.235694	302270.936927	52.377511
3266.349190	302079.113553	52.382516
3265.529536	301886.770038	52.387521
3265.124551	301706.584444	52.392525
3263.999620	301522.132339	52.397530
3263.930944	301323.582898	52.402535
3262.887325	301155.746941	52.407540
3262.013612	300960.966060	52.412545
3261.744343	300774.162146	52.417549
3260.434790	300590.527602	52.422554
3260.135815	300408.439231	52.427559
3259.500719	300232.490297	52.432564
3258.644549	300045.803841	52.437569
3258.420836	299857.998464	52.442573
3257.514184	299684.842274	52.447578
3257.235431	299501.094370	52.452583
3256.544735	299309.924264	52.457588
3255.850735	299118.728996	52.462593
3255.185867	298934.404887	52.467597
3254.628484	298743.391319	52.472602
3253.764799	298557.442925	52.477607
3253.190415	298368.901898	52.482612
3252.550909	298171.992419	52.487617
3251.666182	297992.133298	52.492621
3250.739336	297807.467439	52.497626
3250.409836	297611.858037	52.502631
3249.739119	297429.519684	52.507636
3248.860250	297249.633427	52.512641
3248.164399	297056.908204	52.517645
3247.346127	296878.412677	52.522650
3246.789078	296690.733030	52.527655
3246.358360	296509.985688	52.532660
3245.451748	296328.727718	52.537665
3244.863637	296145.942104	52.542669
3243.872711	295965.894079	52.547674
3243.815415	295770.927305	52.552679
3243.030928	295602.994068	52.557684
3241.946828	295424.997653	52.562689
3241.768832	295225.287091	52.567693
3240.785301	295056.111528	52.572698
3240.195103	294875.897255	52.577703
3239.698972	294692.306275	52.582708
3239.071647	294511.690083	52.587713
3238.175920	294318.433517	52.592717
3237.296168	294148.833321	52.597722
3236.665587	293967.504096	52.602727
3236.004685	293786.790730	52.607732
3235.290494	293610.644293	52.612737
3234.961841	293420.760765	52.617741
3233.993898	293253.236677	52.622746
3233.560439	293064.133446	52.627751
3233.110783	292885.092240	52.632756
3232.567268	292698.425518	52.637761
3231.729147	292515.548965	52.642765
3230.801130	292342.975342	52.647770
3230.197112	292151.045990	52.652775
3229.569390	291964.188265	52.657780
3228.769738	291783.495266	52.662785
3228.096599	291603.138663	52.667789
3227.192927	291435.272032	52.672794
3226.596734	291251.031932	52.677799
3226.317578	291072.446279	52.682804
3225.730569	290885.632234	52.687809
3225.187665	290702.503881	52.692813
3224.300863	290526.739017	52.697818
3223.776445	290342.053961	52.702823
3222.780933	290159.786332	52.707828
3221.915271	289986.640938	52.712833
3221.611366	289807.803666	52.717837
3220.462178	289632.410810	52.722842
3219.904076	289451.576106	52.727847
3219.327516	289279.199501	52.732852
3218.855137	289100.057351	52.737857
3218.115056	288924.904949	52.742861
3217.387475	288750.336225	52.747866
3216.866839	288566.897325	52.752871
3216.223518	288396.237107	52.757876
3215.467386	288213.955836	52.762881
3214.846128	288034.429115	52.767885
3214.076773	287857.090492	52.772890
3213.399539	287683.073489	52.777895
3212.758738	287509.254371	52.782900
3212.041939	287326.584350	52.787905
3211.471175	287149.264856	52.792909
3210.821406	286973.944269	52.797914
3210.257232	286794.204092	52.802919
3209.138226	286622.344802	52.807924
3208.607276	286436.970764	52.812929
3208.284356	286264.348651	52.817933
3207.456650	286088.622818	52.822938
3206.687588	285912.174518	52.827943
3206.165030	285750.611402	52.832948
3205.591603	285573.597163	52.837953
3205.114147	285390.913752	52.842957
3203.869956	285220.601703	52.847962
3203.571159	285024.671930	52.852967
3203.050691	284852.411521	52.857972
3202.352632	284676.690009	52.862977
3201.800292	284496.080959	52.867981
3200.912378	284322.273979	52.872986
3200.428366	284141.373822	52.877991
3199.632802	283968.647221	52.882996
3198.865823	283789.752740	52.888001
3198.484075	283597.426456	52.893005
3197.423813	283431.770747	52.898010
3196.855777	283257.989160	52.903015
3196.518496	283075.715564	52.908020
3195.387344	282899.170509	52.913025
3194.841024	282731.523140	52.918029
3194.049464	282550.900262	52.923034
3193.674386	282371.153754	52.928039
3192.939766	282194.902284	52.933044
3192.217278	282005.940189	52.938049
3191.576910	281831.023512	52.943053
3190.724011	281662.813092	52.948058
3190.175401	281484.825607	52.953063
3189.626013	281306.761790	52.958068
3188.616328	281136.971536	52.963073
3188.263816	280966.491491	52.968077
3187.003944	280796.919014	52.973082
3187.228332	280611.423188	52.978087
3186.454991	280439.150414	52.983092
3185.637162	280272.615008	52.988097
3184.995330	280089.904810	52.993101
3184.286534	279918.665909	52.998106
3183.253950	279742.104386	53.003111
3182.726191	279567.194800	53.008116
3182.251195	279396.046144	53.013121
3181.568819	279226.967736	53.018125
3180.771371	279052.890242	53.023130
3180.392983	278865.018975	53.028135
3179.423963	278685.340061	53.033140
3178.781672	278530.441067	53.038145
3178.565330	278339.971768	53.043149
3177.511960	278172.327186	53.048154
3176.643983	277995.026207	53.053159
3176.348863	277823.237606	53.058164
3175.707608	277650.434080	53.063169
3175.141456	277477.745994	53.068173
3174.352132	277305.271479	53.073178
3173.985718	277125.726229	53.078183
3173.126733	276949.315105	53.083188
3172.130146	276773.740726	53.088193
3171.346637	276593.115348	53.093197
3170.717286	276423.085883	53.098202
3170.259222	276245.872688	53.103207
3169.619508	276080.225406	53.108212
3168.967738	275905.793430	53.113217
3167.836518	275722.828993	53.118221
3167.720947	275559.059824	53.123226
3166.992045	275385.098467	53.128231
3166.191772	275213.567897	53.133236
3165.735042	275046.949305	53.138241
3164.884098	274863.482075	53.143245
3164.115704	274687.718707	53.148250
3163.357156	274517.811514	53.153255
3162.773649	274363.335942	53.158260
3162.133710	274182.993417	53.163265
3161.912797	274017.763757	53.168269
3160.990774	273847.653236	53.173274
3160.198668	273658.777433	53.178279
3159.242082	273491.346581	53.183284
3158.662872	273325.358660	53.188289
3158.256479	273147.959039	53.193293
3157.374828	272979.013731	53.198298
3156.607506	272808.624117	53.203303
3155.908359	272639.395276	53.208308
3155.200242	272474.955926	53.213313
3154.820845	272301.346901	53.218317
3154.088127	272139.585657	53.223322
3153.669495	271972.579186	53.228327
3152.830067	271800.112686	53.233332
3152.155420	271632.178971	53.238337
3151.743261	271460.408960	53.243341
3150.929513	271288.065812	53.248346
3150.575973	271121.864145	53.253351
3149.677448	270953.405653	53.258356
3148.486911	270772.513911	53.263361
3148.456320	270590.139773	53.268365
3147.480294	270433.434537	53.273370
3146.752304	270255.143879	53.278375
3146.371703	270080.261979	53.283380
3145.599085	269921.156096	53.288385
3144.976173	269747.254938	53.293389
3144.220179	269581.219114	53.298394
3143.693437	269405.061605	53.303399
3143.074083	269238.367529	53.308404
3142.342377	269069.526466	53.313409
3141.566681	268891.218206	53.318413
3140.595975	268734.716224	53.323418
3139.929901	268565.228196	53.328423
3139.515695	268389.715318	53.333428
3138.459409	268231.418756	53.338433
3138.047359	268063.342360	53.343437
3137.031452	267900.506149	53.348442
3136.485423	267729.089243	53.353447
3135.983184	267576.257261	53.358452
3135.543231	267413.355521	53.363457
3135.100600	267246.965109	53.368461
3134.398876	267084.359574	53.373466
3133.394997	266902.089526	53.378471
3133.118975	266733.024224	53.383476
3132.320398	266568.091109	53.388481
3131.455892	266396.113802	53.393485
3130.608915	266240.993702	53.398490
3129.968214	266060.831293	53.403495
3129.492940	265908.708663	53.408500
3128.653540	265740.242231	53.413505
3128.204847	265571.128269	53.418509
3127.430116	265417.295896	53.423514
3126.867885	265246.595538	53.428519
3126.279334	265079.923373	53.433524
3125.070649	264913.043791	53.438529
3124.759472	264740.037256	53.443533
3123.820223	264588.294141	53.448538
3123.464029	264416.822954	53.453543
3122.996638	264258.460010	53.458548
3122.010555	264104.101289	53.463553
3121.652209	263922.061436	53.468557
3120.605619	263763.153658	53.473562
3119.884950	263592.275354	53.478567
3119.434998	263435.820103	53.483572
3118.674146	263271.111563	53.488577
3118.077105	263106.046095	53.493581
3117.408521	262955.661562	53.498586
3116.807565	262790.877013	53.503591
3116.455572	262622.513107	53.508596
3115.155315	262463.697006	53.513601
3114.672132	262299.123276	53.518605
3113.981804	262135.168173	53.523610
3113.477037	261970.598028	53.528615
3112.677847	261803.655116	53.533620
3112.327438	261634.170894	53.538625
3111.834605	261479.837193	53.543629
3110.814024	261316.877095	53.548634
3110.147307	261141.712949	53.553639
3109.458099	260984.278041	53.558644
3108.630850	260830.328681	53.563649
3108.474037	260656.866876	53.568653
3107.126647	260502.923602	53.573658
3106.813913	260332.364525	53.578663
3106.199282	260169.519109	53.583668
3105.430255	260007.895204	53.588673
3104.663439	259852.994513	53.593677
3104.159155	259691.532643	53.598682
3103.479003	259525.463589	53.603687
3102.804695	259366.269976	53.608692
3102.127665	259201.142936	53.613697
3101.806476	259030.840701	53.618701
3100.628711	258869.689661	53.623706
3100.171779	258711.353418	53.628711
3099.794623	258544.727696	53.633716
3098.767408	258383.171130	53.638721
3098.264434	258212.847283	53.643725
3097.611923	258060.298068	53.648730
3096.959529	257887.451347	53.653735
3096.214779	257731.275089	53.658740
3095.353599	257569.132509	53.663745
3094.967861	257410.505708	53.668749
3094.194871	257243.052173	53.673754
3093.379715	257079.119934	53.678759
3092.775262	256921.088365	53.683764
3091.766870	256757.518016	53.688769
3091.692892	256596.957856	53.693773
3090.403034	256445.427398	53.698778
3090.085139	256278.997653	53.703783
3089.413653	256121.308338	53.708788
3088.574586	255969.757804	53.713793
3088.150872	255808.336752	53.718797
3087.395836	255645.822232	53.723802
3086.616019	255495.077610	53.728807
3086.353929	255340.329213	53.733812
3085.328277	255180.353668	53.738817
3084.791377	255016.251619	53.743821
3083.867038	254866.294343	53.748826
3083.436150	254705.079020	53.753831
3082.882329	254546.506393	53.758836
3082.195510	254397.021218	53.763841
3081.874721	254226.213238	53.768845
3080.994885	254067.972727	53.773850
3080.406955	253893.183525	53.778855
3079.647941	253738.031137	53.783860
3078.690811	253578.708179	53.788865
3078.252907	253413.063779	53.793869
3077.283362	253266.909458	53.798874
3076.764349	253096.515857	53.803879
3076.185842	252939.552873	53.808884
3075.500339	252794.423578	53.813889
3074.755600	252633.412466	53.818893
3074.264907	252471.062481	53.823898
3073.361829	252307.249901	53.828903
3072.744241	252142.246282	53.833908
3072.031693	251993.480161	53.838913
3071.801155	251826.199971	53.843917
3070.786149	251674.807982	53.848922
3070.298929	251514.139122	53.853927
3069.789259	251350.392498	53.858932
3068.852943	251201.153133	53.863937
3068.347458	251037.991877	53.868941
3067.633197	250878.658340	53.873946
3067.049588	250713.778032	53.878951
3066.391856	250551.176139	53.883956
3065.627889	250393.608119	53.888961
3065.114315	250222.605250	53.893965
3063.910879	250076.999935	53.898970
3063.560989	249915.164872	53.903975
3063.309592	249757.516337	53.908980
3061.931758	249600.784765	53.913985
3061.419031	249439.841806	53.918989
3060.801441	249285.002060	53.923994
3060.117189	249131.828326	53.928999
3059.443323	248971.726267	53.934004
3058.679322	248813.650472	53.939009
3057.896253	248657.436890	53.944013
3056.929249	248504.537719	53.949018
3056.553613	248353.455066	53.954023
3056.183368	248192.949229	53.959028
3055.483855	248057.910877	53.964033
3054.986148	247886.831626	53.969037
3054.472677	247743.411226	53.974042
3053.722824	247586.582300	53.979047
3052.838737	247417.500160	53.984052
3051.997462	247270.948845	53.989057
3051.590225	247099.244996	53.994061
3050.734852	246956.465191	53.999066
3050.086797	246805.121630	54.004071
3049.631166	246643.255822	54.009076
3048.899963	246489.022641	54.014081
3048.193986	246331.780665	54.019085
3047.520095	246173.082232	54.024090
3047.136588	246018.259746	54.029095
3046.343186	245868.391732	54.034100
3045.354836	245714.658478	54.039105
3045.021779	245551.934148	54.044109
3044.217267	245396.287688	54.049114
3043.507236	245238.945717	54.054119
3042.989552	245087.532434	54.059124
3041.920706	244934.474898	54.064129
3041.661622	244781.645883	54.069133
3040.550496	244628.544453	54.074138
3040.193665	244470.434434	54.079143
3039.653937	244322.896252	54.084148
3038.778632	244172.100842	54.089153
3038.336191	244010.439759	54.094157
3037.525368	243858.768677	54.099162
3036.904993	243702.687587	54.104167
3036.317190	243548.180378	54.109172
3035.619742	243398.248993	54.114177
3035.200786	243236.228637	54.119181
3034.190673	243077.892651	54.124186
3033.814837	242918.437859	54.129191
3033.063583	242772.106315	54.134196
3032.543768	242627.138890	54.139201
3031.792040	242468.966487	54.144205
3030.901309	242303.915252	54.149210
3030.097611	242149.698564	54.154215
3029.548580	241994.957922	54.159220
3028.962674	241848.321172	54.164225
3028.545811	241685.054698	54.169229
3027.622711	241539.541216	54.174234
3027.162761	241379.337759	54.179239
3026.349393	241225.352947	54.184244
3025.695568	241071.648655	54.189249
3025.393777	240914.451091	54.194253
3024.522007	240764.117577	54.199258
3023.613013	240600.421170	54.204263
3023.239906	240442.547970	54.209268
3022.279676	240288.613076	54.214273
3021.731278	240124.172707	54.219277
3020.816076	239971.173293	54.224282
3020.074620	239812.009624	54.229287
3019.671514	239658.751310	54.234292
3018.494348	239508.595069	54.239297
3018.349452	239361.356823	54.244301
3017.648880	239208.782806	54.249306
3016.842357	239059.612525	54.254311
3016.490033	238901.712670	54.259316
3015.635024	238754.995042	54.264321
3015.051401	238593.694549	54.269325
3014.189416	238444.992217	54.274330
3013.572422	238300.325575	54.279335
3013.038852	238143.652294	54.284340
3012.348414	237991.485752	54.289345
3011.632243	237829.290641	54.294349
3011.193338	237688.212511	54.299354
3010.252360	237535.424194	54.304359
3009.582381	237393.135286	54.309364
3008.882207	237238.781429	54.314369
3008.396356	237081.490980	54.319373
3007.713214	236925.225082	54.324378
3007.138407	236771.997924	54.329383
3006.524767	236623.564329	54.334388
3005.918339	236474.264031	54.339393
3005.112552	236314.046095	54.344397
3004.344174	236157.489253	54.349402
3003.692387	236002.773035	54.354407
3003.049048	235854.116051	54.359412
3002.496595	235705.393965	54.364417
3001.956575	235536.579384	54.369421
3000.866911	235391.736854	54.374426
3000.269406	235234.619619	54.379431
2999.924529	235089.404983	54.384436
2998.628140	234942.329567	54.389441
2998.363054	234784.320110	54.394445
2997.741205	234644.624574	54.399450
2997.249555	234488.026462	54.404455
2996.282861	234337.920530	54.409460
2995.476310	234199.069675	54.414465
2995.196949	234038.822883	54.419469
2994.518853	233895.139576	54.424474
2993.577945	233735.532721	54.429479
2993.141790	233579.716605	54.434484
2992.033233	233445.396108	54.439489
2991.565420	233292.310002	54.444493
2991.116024	233145.255935	54.449498
2990.431698	232989.683746	54.454503
2989.829421	232837.994634	54.459508
2989.112780	232690.550693	54.464513
2988.491406	232533.874369	54.469517
2987.614942	232391.064949	54.474522
2986.639292	232237.678961	54.479527
2986.325162	232091.190730	54.484532
2985.669133	231947.455885	54.489537
2985.126009	231796.039149	54.494541
2984.717560	231644.168472	54.499546
2983.793855	231497.573957	54.504551
2983.074500	231341.729911	54.509556
2981.950490	231189.489460	54.514561
2981.555449	231040.571279	54.519565
2981.063178	230902.617534	54.524570
2979.968969	230763.689869	54.529575
2979.755668	230618.410168	54.534580
2978.811292	230479.942994	54.539585
2978.033504	230325.968652	54.544589
2977.134693	230192.001507	54.549594
2976.761197	230047.537398	54.554599
2976.699495	229908.829510	54.559604
2975.443175	229769.903558	54.564609
2975.156610	229612.491675	54.569613
2974.453266	229466.400221	54.574618
2973.529070	229314.385885	54.579623
2972.997430	229165.135929	54.584628
2971.961575	229031.523211	54.589633
2971.618702	228883.415088	54.594637
2970.959311	228734.848085	54.599642
2970.010241	228584.748567	54.604647
2969.666731	228442.013701	54.609652
2968.860273	228307.067222	54.614657
2968.743966	228156.862063	54.619661
2967.899815	228025.002837	54.624666
2966.951782	227868.971850	54.629671
2966.270953	227722.141344	54.634676
2965.583172	227572.027668	54.639681
2965.135919	227430.685802	54.644685
2964.200889	227285.143890	54.649690
2963.583937	227148.361467	54.654695
2963.126216	227000.274735	54.659700
2962.302714	226863.576391	54.664705
2961.942047	226702.896992	54.669709
2961.101253	226566.023639	54.674714
2960.387483	226420.779176	54.679719
2959.944588	226278.521940	54.684724
2959.469674	226128.237082	54.689729
2958.529528	225981.717980	54.694733
2957.326473	225827.080551	54.699738
2957.122332	225690.617058	54.704743
2956.413159	225547.868549	54.709748
2955.559496	225407.307324	54.714753
2955.402168	225258.348644	54.719757
2954.411747	225118.318779	54.724762
2953.543612	224974.578006	54.729767
2953.148603	224829.540477	54.734772
2952.444790	224680.592986	54.739777
2951.931825	224535.867452	54.744781
2951.343844	224391.726912	54.749786
2950.514517	224239.477520	54.754791
2949.983679	224094.831987	54.759796
2949.100593	223959.344533	54.764801
2948.838186	223802.512478	54.769805
2947.835915	223659.788236	54.774810
2946.996098	223515.931015	54.779815
2946.437122	223371.227601	54.784820
2945.719114	223216.836621	54.789825
2945.127430	223077.727403	54.794829
2944.503616	222940.189304	54.799834
2943.659194	222798.319999	54.804839
2943.275308	222648.421833	54.809844
2941.958654	222515.997035	54.814849
2941.596619	222358.127047	54.819853
2940.909455	222224.890211	54.824858
2940.388736	222086.968132	54.829863
2939.986094	221942.891835	54.834868
2939.320426	221802.854605	54.839873
2938.709074	221650.881240	54.844877
2937.995914	221515.600256	54.849882
2936.933651	221369.058064	54.854887
2936.469334	221222.968862	54.859892
2935.505903	221090.019605	54.864897
2935.078310	220942.944944	54.869901
2934.061400	220803.728942	54.874906
2933.534386	220666.599667	54.879911
2933.030242	220526.857459	54.884916
2932.305447	220397.321359	54.889921
2932.074481	220251.337122	54.894925
2931.203832	220117.305618	54.899930
2930.516723	219959.581190	54.904935
2929.985008	219814.523761	54.909940
2928.842202	219687.740995	54.914945
2928.519513	219535.649832	54.919949
2927.837030	219397.949230	54.924954
2927.291492	219252.500485	54.929959
2926.480234	219110.187328	54.934964
2925.512310	218969.719543	54.939969
2925.222092	218828.113659	54.944973
2924.091715	218693.871290	54.949978
2923.265795	218558.104374	54.954983
2922.889937	218416.882000	54.959988
2921.993631	218284.767298	54.964993
2921.762341	218146.221153	54.969997
2921.307472	218012.293164	54.975002
2920.530499	217876.507056	54.980007
2919.772765	217732.304233	54.985012
2919.398027	217587.519170	54.990017
2918.885785	217443.812682	54.995021
2918.007345	217297.236794	55.000026
2917.383852	217155.037802	55.005031
2916.695568	217008.012350	55.010036
2915.595295	216879.776700	55.015041
2915.184538	216738.715928	55.020045
2914.679489	216600.470725	55.025050
2913.765410	216461.463182	55.030055
2913.273537	216322.732747	55.035060
2912.336232	216178.739744	55.040065
2912.152254	216045.790905	55.045069
2911.206227	215905.605758	55.050074
2910.600041	215768.014663	55.055079
2910.134725	215619.213006	55.060084
2909.174375	215483.167816	55.065089
2908.422489	215339.007194	55.070093
2908.106510	215205.737205	55.075098
2907.401204	215058.209443	55.080103
2906.778847	214908.097694	55.085108
2905.819579	214767.942432	55.090113
2905.746957	214627.061560	55.095117
2904.813599	214484.713476	55.100122
2903.859415	214341.274343	55.105127
2903.457929	214205.703279	55.110132
2902.480644	214065.883270	55.115137
2901.727880	213918.721909	55.120141
2901.294206	213787.344427	55.125146
2900.557866	213646.710716	55.130151
2899.888024	213505.175791	55.135156
2898.956836	213374.679784	55.140161
2898.633931	213238.130896	55.145165
2897.860954	213101.538999	55.150170
2897.076325	212959.374279	55.155175
2896.519873	212821.895889	55.160180
2895.887482	212685.193501	55.165185
2895.303897	212549.272813	55.170189
2894.434737	212416.528739	55.175194
2894.053217	212265.201109	55.180199
2893.032532	212135.994546	55.185204
2892.254120	212003.924260	55.190209
2891.730353	211861.542435	55.195213
2891.109903	211735.671671	55.200218
2890.197686	211603.534295	55.205223
2889.831571	211460.912016	55.210228
2889.085598	211339.376665	55.215233
2888.467508	211199.276804	55.220237
2887.833539	211063.774512	55.225242
2887.090899	210928.416992	55.230247
2886.481114	210795.215174	55.235252
2885.624754	210670.172983	55.240257
2885.491761	210522.221145	55.245261
2884.998204	210385.603481	55.250266
2883.715781	210244.949079	55.255271
2883.404432	210104.777609	55.260276
2882.742172	209973.253153	55.265281
2881.999605	209830.299592	55.270285
2881.227078	209697.584055	55.275290
2880.708445	209559.432126	55.280295
2880.256287	209416.000793	55.285300
2879.226044	209288.265205	55.290305
2878.680259	209146.058431	55.295309
2877.998978	209020.164528	55.300314
2876.938575	208879.134413	55.305319
2876.837018	208737.570969	55.310324
2876.186300	208601.173013	55.315329
2875.511490	208461.100985	55.320333
2874.583778	208326.249324	55.325338
2873.830762	208186.648489	55.330343
2873.785369	208051.034086	55.335348
2872.739489	207917.563852	55.340353
2872.129339	207773.728642	55.345357
2871.368503	207637.210279	55.350362
2870.650160	207504.121813	55.355367
2869.933519	207370.346108	55.360372
2868.945786	207245.509832	55.365377
2868.303776	207104.773933	55.370381
2867.957072	206983.082084	55.375386
2867.220362	206840.185486	55.380391
2867.134779	206699.553331	55.385396
2866.081871	206570.541623	55.390401
2865.504060	206436.147855	55.395405
2864.728177	206307.423749	55.400410
2864.052066	206166.911817	55.405415
2863.571855	206024.027467	55.410420
2862.831491	205892.358752	55.415425
2862.249269	205755.256428	55.420429
2861.576956	205617.799615	55.425434
2861.107087	205472.445985	55.430439
2860.303061	205328.023769	55.435444
2859.512478	205200.907964	55.440449
2858.797057	205060.990323	55.445453
2858.053997	204929.056939	55.450458
2857.392492	204797.861805	55.455463
2856.927625	204657.510935	55.460468
2855.812834	204528.857129	55.465473
2855.268109	204388.354113	55.470477
2854.801382	204259.623734	55.475482
2853.747706	204117.496636	55.480487
2853.470994	203987.756844	55.485492
2852.507308	203861.842216	55.490497
2852.146063	203724.595155	55.495501
2851.460561	203588.379693	55.500506
2850.812382	203447.093609	55.505511
2850.350840	203314.928451	55.510516
2849.391546	203186.163952	55.515521
2849.063713	203045.388087	55.520525
2847.968159	202920.336349	55.525530
2847.004337	202782.767021	55.530535
2846.708205	202646.072200	55.535540
2846.021740	202522.661849	55.540545
2845.553495	202392.523344	55.545549
2844.693232	202262.536302	55.550554
2843.938572	202123.204736	55.555559
2843.659252	201994.946124	55.560564
2842.593482	201859.991286	55.565569
2842.167244	201718.954357	55.570573
2841.519194	201591.989471	55.575578
2840.696643	201453.866555	55.580583
2840.160157	201316.055002	55.585588
2839.277226	201197.247238	55.590593
2838.940475	201061.873477	55.595597
2838.293926	200930.150467	55.600602
2837.583627	200790.827948	55.605607
2836.674113	200656.462132	55.610612
2836.142548	200533.820659	55.615617
2835.695551	200391.008832	55.620621
2834.887196	200265.332217	55.625626
2834.119457	200132.103259	55.630631
2833.258522	199995.097207	55.635636
2832.426778	199870.990435	55.640641
2831.976869	199730.102339	55.645645
2831.576921	199604.528005	55.650650
2830.703003	199474.040701	55.655655
2830.364476	199340.771166	55.660660
2829.481186	199218.850079	55.665665
2828.737397	199081.395132	55.670669
2828.376002	198957.050547	55.675674
2827.479331	198817.139078	55.680679
2827.256540	198687.403154	55.685684
2826.291397	198557.734208	55.690689
2825.684999	198414.863777	55.695693
2824.999964	198280.684650	55.700698
2824.451342	198149.449183	55.705703
2823.697081	198015.358041	55.710708
2823.014119	197886.842192	55.715713
2822.562018	197753.098334	55.720717
2821.640883	197612.035948	55.725722
2820.899631	197469.558445	55.730727
2820.661184	197337.206988	55.735732
2819.642982	197207.677006	55.740737
2819.056469	197074.897792	55.745741
2818.504719	196945.307312	55.750746
2817.680406	196814.487851	55.755751
2817.305873	196674.333949	55.760756
2816.422665	196534.859041	55.765761
2815.602532	196399.611800	55.770765
2815.130722	196262.515587	55.775770
2814.100155	196143.004426	55.780775
2814.164331	195997.731241	55.785780
2812.974946	195865.330537	55.790785
2812.325918	195736.954580	55.795789
2811.916885	195598.895857	55.800794
2810.744496	195464.623012	55.805799
2810.118223	195333.165170	55.810804
2809.267513	195204.148100	55.815809
2809.059083	195069.660003	55.820813
2808.625078	194942.473511	55.825818
2807.586635	194807.366832	55.830823
2807.157066	194674.721634	55.835828
2806.085998	194545.766581	55.840833
2805.724183	194414.014747	55.845837
2804.785532	194295.294970	55.850842
2804.293569	194154.288594	55.855847
2803.616911	194022.040514	55.860852
2802.921179	193894.223736	55.865857
2802.840002	193762.734531	55.870861
2801.756979	193626.849191	55.875866
2801.077901	193498.916268	55.880871
2800.557843	193364.736542	55.885876
2799.651445	193226.699440	55.890881
2799.139806	193091.068606	55.895885
2798.456957	192959.460502	55.900890
2797.976978	192833.597166	55.905895
2797.606387	192685.692198	55.910900
2796.742982	192562.867609	55.915905
2796.008608	192420.873909	55.920909
2795.333735	192286.619828	55.925914
2794.689170	192156.649133	55.930919
2794.267554	192018.933049	55.935924
2793.204850	191889.398267	55.940929
2792.697385	191743.095512	55.945933
2791.956426	191615.508070	55.950938
2791.284250	191484.105791	55.955943
2790.838542	191340.873505	55.960948
2789.893051	191203.827959	55.965953
2789.531919	191066.104979	55.970957
2788.846230	190931.983562	55.975962
2788.097356	190800.111799	55.980967
2787.597259	190660.249046	55.985972
2786.924572	190528.404126	55.990977
2786.433317	190377.662560	55.995981
2785.110664	190243.045959	56.000986
2784.682753	190101.748417	56.005991
2784.083978	189972.132557	56.010996
2783.092239	189841.243383	56.016001
2782.594885	189711.688502	56.021005
2782.177966	189579.474884	56.026010
2781.208138	189436.114982	56.031015
2780.045163	189298.689461	56.036020
2779.710272	189179.606566	56.041025
2779.110483	189050.311440	56.046029
2778.653212	188922.164577	56.051034
2777.600041	188787.802028	56.056039
2777.491112	188655.745761	56.061044
2776.745536	188532.162136	56.066049
2776.059523	188392.997048	56.071053
2775.410914	188262.414116	56.076058
2774.409080	188130.615250	56.081063
2773.830322	188008.393326	56.086068
2773.217958	187870.592142	56.091073
2773.121384	187733.002280	56.096077
2772.056529	187600.731442	56.101082
2771.166773	187466.664851	56.106087
2770.732239	187330.465544	56.111092
2770.104349	187210.568936	56.116097
2769.496756	187065.568620	56.121101
2768.867224	186941.894489	56.126106
2767.817548	186805.501549	56.131111
2767.475160	186665.841917	56.136116
2766.771563	186537.091788	56.141121
2766.307272	186402.719171	56.146125
2765.516526	186269.263745	56.151130
2764.787737	186141.689131	56.156135
2764.312652	185994.826520	56.161140
2763.511285	185866.818902	56.166145
2762.879275	185729.383423	56.171149
2762.401010	185604.289538	56.176154
2761.510057	185470.890480	56.181159
2761.131037	185329.052591	56.186164
2759.957169	185198.383418	56.191169
2759.691529	185059.785148	56.196173
2758.878275	184925.370381	56.201178
2758.060010	184789.773707	56.206183
2757.479299	184644.916743	56.211188
2756.609698	184523.131805	56.216193
2756.209701	184384.874923	56.221197
2755.627973	184253.491345	56.226202
2754.926801	184113.018601	56.231207
2754.176038	183978.062470	56.236212
2753.586084	183853.512699	56.241217
2752.998630	183712.005502	56.246221
2752.285793	183579.194453	56.251226
2751.706431	183445.510342	56.256231
2750.946162	183308.051680	56.261236
2750.163294	183180.379516	56.266241
2749.393395	183039.335874	56.271245
2748.649991	182906.455352	56.276250
2748.334922	182778.188689	56.281255
2747.732511	182638.684470	56.286260
2746.999412	182514.669965	56.291265
2746.609310	182370.884195	56.296269
2745.787656	182236.160848	56.301274
2745.093878	182100.883387	56.306279
2744.686709	181967.914276	56.311284
2743.917772	181834.875666	56.316289
2743.240769	181695.526187	56.321293
2742.346918	181556.071575	56.326298
2741.684971	181412.739070	56.331303
2741.257394	181274.330910	56.336308
2740.354483	181157.407034	56.341313
2739.821912	181012.503458	56.346317
2739.046038	180879.990405	56.351322
2738.137408	180739.141516	56.356327
2737.776309	180604.146739	56.361332
2736.920126	180462.247380	56.366337
2736.602274	180333.861139	56.371341
2735.903947	180193.642172	56.376346
2734.955331	180076.410461	56.381351
2734.450833	179929.152850	56.386356
2733.594995	179809.973715	56.391361
2733.260168	179660.909339	56.396365
2732.776461	179524.182014	56.401370
2731.644057	179389.427719	56.406375
2731.279626	179246.971132	56.411380
2730.569730	179129.348050	56.416385
2730.143063	178978.965020	56.421389
2729.489568	178847.392857	56.426394
2728.457230	178708.452783	56.431399
2728.182061	178564.979486	56.436404
2727.064344	178427.478467	56.441409
2726.493999	178286.596807	56.446413
2725.921598	178160.750486	56.451418
2725.000929	178033.903989	56.456423
2724.758953	177882.172777	56.461428
2723.753611	177747.543508	56.466433
2722.958736	177609.485248	56.471437
2722.542921	177480.334556	56.476442
2721.718661	177349.811681	56.481447
2721.617267	177202.703220	56.486452
2720.711939	177070.222572	56.491457
2720.270011	176928.600144	56.496461
2719.462410	176784.148876	56.501466
2718.508666	176653.559664	56.506471
2718.195768	176518.379511	56.511476
2717.527704	176374.492646	56.516481
2716.712504	176239.075001	56.521485
2715.768670	176107.926310	56.526490
2715.340225	175968.479975	56.531495
2714.670605	175830.738490	56.536500
2714.033782	175703.510742	56.541505
2713.352106	175557.708346	56.546509
2712.920459	175418.111762	56.551514
2712.152888	175286.454463	56.556519
2711.485801	175136.123403	56.561524
2710.916210	175001.116093	56.566529
2710.545736	174861.028417	56.571533
2709.735225	174735.510051	56.576538
2708.800747	174584.625616	56.581543
2708.273171	174446.179505	56.586548
2707.272378	174311.764253	56.591553
2706.768456	174160.062809	56.596557
2706.523805	174022.489049	56.601562
2705.477666	173892.215827	56.606567
2705.171919	173743.753147	56.611572
2704.252474	173610.904405	56.616577
2704.020133	173466.602681	56.621581
2703.036923	173316.888062	56.626586
2702.537651	173172.591528	56.631591
2702.176275	173024.407402	56.636596
2701.244728	172880.460200	56.641601
2700.376267	172740.636840	56.646605
2699.759257	172592.914505	56.651610
2698.746265	172453.890840	56.656615
2698.283790	172310.303796	56.661620
2697.491468	172187.448536	56.666625
2697.111286	172040.822615	56.671629
2696.363744	171909.071472	56.676634
2695.567565	171765.119591	56.681639
2695.508594	171602.700042	56.686644
2694.447556	171468.812620	56.691649
2693.798598	171323.147606	56.696653
2693.394263	171186.804382	56.701658
2692.523753	171045.156044	56.706663
2691.661850	170891.730632	56.711668
2690.908096	170753.142443	56.716673
2690.379393	170607.753536	56.721677
2689.861960	170472.880480	56.726682
2688.804536	170335.473712	56.731687
2688.716186	170191.873293	56.736692
2687.800480	170057.942251	56.741697
2686.938663	169909.454904	56.746701
2686.491341	169769.944200	56.751706
2685.682598	169634.471645	56.756711
2685.078668	169487.115018	56.761716
2684.095981	169353.146161	56.766721
2683.822109	169204.136009	56.771725
2683.308517	169068.504232	56.776730
2682.441686	168933.933513	56.781735
2682.160758	168778.694964	56.786740
2681.223603	168635.959653	56.791745
2680.445361	168493.199699	56.796749
2680.158601	168346.178697	56.801754
2679.316585	168209.152318	56.806759
2678.567863	168062.434493	56.811764
2677.891494	167915.807501	56.816769
2677.332029	167776.372681	56.821773
2676.812305	167627.509353	56.826778
2675.824442	167492.708571	56.831783
2675.596525	167346.826566	56.836788
2674.884215	167204.531504	56.841793
2674.211825	167053.164122	56.846797
2673.349593	166902.323347	56.851802
2672.836511	166760.977526	56.856807
2672.271744	166605.792828	56.861812
2671.470695	166470.724504	56.866817
2670.740488	166313.583555	56.871821
2670.241330	166169.338557	56.876826
2669.483023	166030.335889	56.881831
2669.008755	165877.225244	56.886836
2668.342877	165731.088293	56.891841
2667.431698	165596.803511	56.896845
2666.936557	165433.957894	56.901850
2666.053776	165288.632690	56.906855
2665.540953	165147.572673	56.911860
2664.720484	165002.505742	56.916865
2664.117176	164854.378737	56.921869
2663.295003	164707.520380	56.926874
2662.634568	164567.604902	56.931879
2662.140626	164423.035269	56.936884
2661.332914	164269.958664	56.941889
2661.031253	164131.183220	56.946893
2660.502157	163984.726339	56.951898
2659.624945	163839.812845	56.956903
2659.058275	163692.002590	56.961908
2658.414458	163538.229185	56.966913
2657.807223	163384.819361	56.971917
2657.194320	163242.511033	56.976922
2656.248147	163099.950913	56.981927
2655.817349	162945.624957	56.986932
2655.269108	162790.606248	56.991937
2654.339836	162643.773147	56.996941
2653.664144	162496.341028	57.001946
2652.720523	162349.956399	57.006951
2652.368720	162202.575877	57.011956
2651.664817	162062.804044	57.016961
2651.105306	161914.237035	57.021965
2650.474475	161765.300514	57.026970
2649.584825	161611.141958	57.031975
2649.340597	161457.479366	57.036980
2648.777178	161319.239286	57.041985
2647.816120	161167.369769	57.046989
2647.434499	161006.903464	57.051994
2646.426243	160862.632942	57.056999
2646.020387	160704.422196	57.062004
2645.131126	160555.366380	57.067009
2644.581506	160413.173641	57.072013
2643.743702	160256.991238	57.077018
2643.048501	160117.276490	57.082023
2642.420282	159952.544098	57.087028
2641.735738	159807.349341	57.092033
2641.181556	159660.812327	57.097037
2640.292567	159520.800092	57.102042
2639.397337	159370.199180	57.107047
2639.203894	159216.093268	57.112052
2638.327687	159070.525091	57.117057
2637.961681	158918.418380	57.122061
2637.539678	158770.936067	57.127066
2636.458665	158626.101410	57.132071
2636.120211	158478.009580	57.137076
2635.163450	158329.812938	57.142081
2634.292407	158176.467327	57.147085
2633.836741	158024.861801	57.152090
2632.984669	157876.002149	57.157095
2632.412886	157724.238354	57.162100
2631.698787	157588.820879	57.167105
2631.519111	157437.695408	57.172109
2630.807797	157292.426351	57.177114
2629.795298	157143.518991	57.182119
2629.244271	156991.666132	57.187124
2628.555746	156846.357205	57.192129
2627.956709	156701.454220	57.197133
2627.309931	156544.292021	57.202138
2626.148456	156410.589949	57.207143
2625.913214	156250.300232	57.212148
2625.112170	156102.546112	57.217153
2624.545930	155959.992812	57.222157
2624.185190	155801.860713	57.227162
2623.150785	155652.391255	57.232167
2622.767808	155505.399756	57.237172
2622.548286	155360.785536	57.242177
2621.333125	155205.728033	57.247181
2620.883220	155051.744887	57.252186
2620.076160	154903.132526	57.257191
2619.824186	154739.394982	57.262196
2618.559697	154597.708021	57.267201
2617.811435	154440.241111	57.272205
2617.517010	154290.075678	57.277210
2616.842671	154149.072492	57.282215
2616.145850	153985.116732	57.287220
2615.468579	153841.674718	57.292225
2615.109213	153678.378817	57.297229
2614.222899	153528.348709	57.302234
2613.248875	153370.236181	57.307239
2612.867513	153218.347893	57.312244
2612.428076	153080.515169	57.317249
2611.453176	152925.633486	57.322253
2610.926527	152768.940101	57.327258
2610.242828	152621.500410	57.332263
2609.878828	152460.867764	57.337268
2608.793022	152312.400036	57.342273
2608.406623	152151.251298	57.347277
2607.722783	152005.301517	57.352282
2607.093708	151842.171752	57.357287
2606.645186	151677.412662	57.362292
2605.817236	151531.157340	57.367297
2605.134497	151380.431029	57.372301
2604.508338	151215.410060	57.377306
2603.774472	151063.841712	57.382311
2603.479959	150904.476652	57.387316
2602.343791	150744.686491	57.392321
2601.774369	150585.201316	57.397325
2601.155641	150437.773811	57.402330
2600.402752	150283.733641	57.407335
2599.799964	150112.791696	57.412340
2599.331315	149982.335575	57.417345
2598.490724	149752.561355	57.422349
2597.993771	149589.815877	57.427354
2596.948616	149430.043166	57.432359
2596.621986	149278.647362	57.437364
2595.808869	149119.424055	57.442369
2595.128996	148960.688797	57.447373
2594.723952	148799.051162	57.452378
2593.830675	148653.543551	57.457383
2593.478640	148484.896268	57.462388
2592.780223	148332.979193	57.467393
2591.655123	148175.373223	57.472397
2591.604868	148014.356895	57.477402
2590.273586	147852.159096	57.482407
2589.709068	147694.110812	57.487412
2589.073541	147543.420284	57.492417
2588.237410	147389.076705	57.497421
2587.980865	147229.266232	57.502426
2586.964383	147077.558034	57.507431
2586.605154	146928.618555	57.512436
2585.858901	146768.430492	57.517441
2585.168342	146619.087463	57.522445
2584.827537	146458.531712	57.527450
2584.154600	146301.918167	57.532455
2583.435925	146133.798928	57.537460
2582.833737	145985.270929	57.542465
2582.051385	145820.302387	57.547469
2581.709495	145662.661028	57.552474
2580.587685	145505.868412	57.557479
2580.343205	145347.857370	57.562484
2579.385716	145187.050003	57.567489
2578.901775	145020.386346	57.572493
2578.225358	144863.462826	57.577498
2577.452787	144695.626693	57.582503
2577.150245	144534.769723	57.587508
2575.959601	144390.879169	57.592513
2575.414697	144217.634222	57.597517
2575.208246	144056.523053	57.602522
2574.104827	143898.896907	57.607527
2573.549046	143736.508482	57.612532
2573.046387	143580.707558	57.617537
2572.357115	143421.391684	57.622541
2571.410369	143256.310277	57.627546
2570.900364	143092.863288	57.632551
2570.381302	142938.758241	57.637556
2569.865723	142773.115522	57.642561
2569.094954	142604.515317	57.647565
2568.281163	142441.602792	57.652570
2567.316638	142281.586740	57.657575
2567.029368	142123.319368	57.662580
2566.288519	141965.162815	57.667585
2565.439829	141801.916149	57.672589
2564.876447	141649.235035	57.677594
2564.322008	141487.391957	57.682599
2563.772728	141315.231387	57.687604
2563.428503	141163.102471	57.692609
2562.593940	140993.517480	57.697613
2561.872134	140820.332444	57.702618
2560.841873	140662.914660	57.707623
2560.556818	140489.420886	57.712628
2559.715776	140330.310365	57.717633
2559.081627	140162.134043	57.722637
2558.389171	140006.521200	57.727642
2557.835626	139839.617188	57.732647
2557.138014	139679.928322	57.737652
2556.159619	139522.279578	57.742657
2555.635489	139355.919931	57.747661
2554.986889	139195.895533	57.752666
2554.032504	139035.717165	57.757671
2553.584189	138865.358748	57.762676
2553.177917	138718.359542	57.767681
2552.438595	138548.633492	57.772685
2551.957462	138389.806570	57.777690
2551.329381	138229.415656	57.782695
2550.441996	138052.944128	57.787700
2550.108505	137894.642766	57.792705
2549.079393	137724.370224	57.797709
2548.703320	137551.682907	57.802714
2547.990096	137401.956530	57.807719
2547.243795	137234.716518	57.812724
2546.504527	137065.596071	57.817729
2545.715879	136899.279399	57.822733
2545.198530	136740.886316	57.827738
2544.539910	136572.340325	57.832743
2544.016174	136406.098800	57.837748
2543.359633	136251.948220	57.842753
2542.650838	136081.786869	57.847757
2542.448137	135908.853046	57.852762
2541.269196	135749.642782	57.857767
2540.523212	135584.495579	57.862772
2539.951218	135417.505092	57.867777
2539.690445	135246.146970	57.872781
2538.818305	135083.664979	57.877786
2537.822099	134917.544927	57.882791
2537.374288	134739.016509	57.887796
2536.381999	134592.029192	57.892801
2535.731455	134431.992907	57.897805
2535.360240	134260.162686	57.902810
2534.655184	134094.433131	57.907815
2534.096620	133920.919688	57.912820
2533.176691	133761.399835	57.917825
2532.723688	133594.528042	57.922829
2532.159693	133428.005086	57.927834
2531.347112	133273.056691	57.932839
2530.918566	133099.197330	57.937844
2530.125989	132934.618887	57.942849
2529.236300	132776.293779	57.947853
2528.800118	132602.121084	57.952858
2527.991142	132440.495084	57.957863
2527.243075	132279.266825	57.962868
2526.597004	132112.535901	57.967873
2526.100652	131940.002693	57.972877
2525.504568	131788.965752	57.977882
2524.722966	131629.105635	57.982887
2524.144510	131455.127645	57.987892
2523.600201	131289.528615	57.992897
2522.816971	131124.641625	57.997901
2522.076612	130959.926629	58.002906
2521.180181	130793.128841	58.007911
2520.751791	130626.613506	58.012916
2520.012874	130471.630626	58.017921
2519.429314	130294.154965	58.022925
2519.067842	130132.077489	58.027930
2518.180860	129975.418823	58.032935
2517.697782	129802.871185	58.037940
2516.815398	129633.626713	58.042945
2516.177253	129463.747602	58.047949
2515.360792	129296.069672	58.052954
2514.496636	129131.791477	58.057959
2514.243966	128974.567955	58.062964
2513.570760	128816.510215	58.067969
2512.764826	128642.928657	58.072973
2512.209616	128481.412212	58.077978
2511.069263	128318.668589	58.082983
2510.626815	128142.213016	58.087988
2509.935192	127992.684964	58.092993
2509.577668	127820.294840	58.097997
2508.700458	127657.081594	58.103002
2508.206156	127497.224991	58.108007
2507.745446	127324.041510	58.113012
2506.895767	127169.221608	58.118017
2506.251753	127002.063658	58.123021
2505.627448	126836.351396	58.128026
2505.116981	126684.731650	58.133031
2504.414316	126501.901707	58.138036
2503.635609	126336.001051	58.143041
2502.950474	126177.960348	58.148045
2502.091190	126007.070808	58.153050
2501.009766	125844.091229	58.158055
2501.091322	125676.978774	58.163060
2500.408274	125514.547597	58.168065
2499.805990	125346.199438	58.173069
2499.131786	125177.266863	58.178074
2498.352414	125020.568541	58.183079
2497.693980	124839.025374	58.188084
2497.297267	124670.991702	58.193089
2496.483304	124501.615640	58.198093
2495.931661	124331.068871	58.203098
2495.072738	124169.105411	58.208103
2494.527120	123991.943815	58.213108
2493.688008	123823.769674	58.218113
2493.135289	123655.500398	58.223117
2492.580804	123483.651516	58.228122
2491.693818	123324.808702	58.233127
2491.365033	123150.919849	58.238132
2490.253472	122980.546606	58.243137
2489.710232	122806.706685	58.248141
2489.083868	122633.617555	58.253146
2488.474534	122462.901355	58.258151
2487.746814	122299.417373	58.263156
2487.140554	122134.696161	58.268161
2486.154211	121964.957158	58.273165
2485.783001	121793.407565	58.278170
2485.141191	121634.993087	58.283175
2484.337333	121466.091786	58.288180
2483.847393	121301.052583	58.293185
2483.237912	121139.994904	58.298189
2482.523176	120979.424688	58.303194
2481.712615	120806.935368	58.308199
2481.478762	120631.981423	58.313204
2480.537456	120462.308432	58.318209
2479.657506	120309.221595	58.323213
2479.464927	120124.944995	58.328218
2478.873277	119962.571241	58.333223
2478.197089	119784.950576	58.338228
2477.487136	119612.802321	58.343233
2476.971997	119439.049962	58.348237
2476.411119	119262.620733	58.353242
2475.083648	119096.001464	58.358247
2474.828178	118912.517859	58.363252
2473.871999	118751.066423	58.368257
2473.064549	118582.723872	58.373261
2472.770343	118411.622215	58.378266
2472.119073	118248.881373	58.383271
2471.177087	118074.723358	58.388276
2470.700133	117903.247765	58.393281
2470.039586	117728.920513	58.398285
2469.489801	117566.409100	58.403290
2468.535276	117405.022938	58.408295
2468.585990	117217.681489	58.413300
2467.737365	117053.576638	58.418305
2466.638662	116872.831015	58.423309
2466.191507	116688.784223	58.428314
2465.297913	116523.369606	58.433319
2464.843753	116359.333620	58.438324
2464.187995	116180.934702	58.443329
2463.575400	116011.619625	58.448333
2463.035575	115834.067996	58.453338
2462.271752	115664.207939	58.458343
2461.752275	115491.511147	58.463348
2461.248627	115328.003767	58.468353
2460.277667	115145.314237	58.473357
2459.849200	114971.172098	58.478362
2459.008691	114801.755223	58.483367
2458.111097	114624.338584	58.488372
2457.494470	114453.676268	58.493377
2457.003808	114277.409830	58.498381
2456.669479	114096.461220	58.503386
2455.474063	113930.990749	58.508391
2455.217018	113746.852625	58.513396
2454.385179	113574.992749	58.518401
2453.448080	113406.171774	58.523405
2453.108540	113220.622573	58.528410
2452.113348	113064.741283	58.533415
2451.704195	112889.550583	58.538420
2451.171398	112718.340954	58.543425
2450.497814	112538.917059	58.548429
2449.691306	112363.773996	58.553434
2448.891404	112191.772591	58.558439
2448.638256	112010.521546	58.563444
2447.919648	111839.264907	58.568449
2447.118861	111669.875590	58.573453
2446.588099	111491.864515	58.578458
2445.848177	111316.001155	58.583463
2445.135546	111130.710697	58.588468
2444.387658	110960.048619	58.593473
2443.900112	110786.040155	58.598477
2443.479445	110602.065431	58.603482
2442.507904	110431.753416	58.608487
2442.065467	110247.607102	58.613492
2441.544686	110075.163674	58.618497
2440.353758	109894.996947	58.623501
2439.846490	109717.109175	58.628506
2439.120097	109548.350865	58.633511
2438.538691	109366.416122	58.638516
2437.608091	109196.709028	58.643521
2437.114465	109018.195952	58.648525
2436.754961	108842.962604	58.653530
2435.284904	108675.946328	58.658535
2434.813985	108502.465414	58.663540
2434.492389	108325.497465	58.668545
2433.865271	108152.792565	58.673549
2433.248086	107980.061937	58.678554
2432.547992	107809.065253	58.683559
2432.093576	107628.119571	58.688564
2431.435632	107458.343310	58.693569
2430.617929	107274.723088	58.698573
2429.946261	107094.469388	58.703578
2429.052595	106932.107196	58.708583
2428.508098	106754.399278	58.713588
2428.126469	106575.822971	58.718593
2427.074920	106406.179967	58.723597
2426.694086	106224.528860	58.728602
2425.945995	106054.992504	58.733607
2425.561773	105881.611830	58.738612
2424.899713	105698.112206	58.743617
2424.056225	105520.473511	58.748621
2423.738306	105338.616115	58.753626
2422.782600	105158.961272	58.758631
2422.106699	104977.689980	58.763636
2421.408937	104805.147201	58.768641
2420.712453	104625.042897	58.773645
2420.264420	104439.514180	58.778650
2419.456081	104268.109441	58.783655
2418.680198	104084.449959	58.788660
2417.965686	103914.796614	58.793665
2417.303563	103742.725381	58.798669
2416.937302	103550.941613	58.803674
2415.743677	103380.257835	58.808679
2415.323211	103199.289532	58.813684
2414.890587	103026.736703	58.818689
2414.211573	102853.386797	58.823693
2413.427915	102673.431709	58.828698
2412.681150	102493.890845	58.833703
2412.309265	102310.656912	58.838708
2411.743479	102145.947244	58.843713
2410.699599	101959.910800	58.848717
2410.350749	101777.444974	58.853722
2409.704870	101612.739069	58.858727
2409.089165	101419.838669	58.863732
2408.384950	101242.812712	58.868737
2407.527491	101061.511517	58.873741
2406.876183	100881.910807	58.878746
2406.169933	100696.103680	58.883751
2405.707789	100518.917984	58.888756
2404.802082	100345.692398	58.893761
2403.961845	100173.371153	58.898765
2403.457325	99995.974158	58.903770
2402.792170	99822.378160	58.908775
2402.175588	99637.123504	58.913780
2401.579008	99461.603731	58.918785
2400.875349	99288.189115	58.923789
2400.169115	99101.792204	58.928794
2399.418193	98924.937256	58.933799
2399.068208	98754.889404	58.938804
2398.317036	98570.292609	58.943809
2397.279471	98394.895290	58.948813
2397.055040	98221.660107	58.953818
2395.835597	98047.873615	58.958823
2395.443327	97866.225663	58.963828
2394.741097	97689.454981	58.968833
2394.011715	97515.049384	58.973837
2393.570352	97342.743204	58.978842
2392.965162	97172.836363	58.983847
2392.706767	96986.652050	58.988852
2391.429923	96807.334555	58.993857
2390.846698	96629.811179	58.998861
2390.300994	96453.615106	59.003866
2389.743713	96279.952759	59.008871
2389.194711	96103.132060	59.013876
2388.605200	95928.272519	59.018881
2388.127072	95737.275283	59.023885
2387.405665	95554.607168	59.028890
2386.457188	95379.485353	59.033895
2385.607339	95198.172294	59.038900
2385.013449	95023.098499	59.043905
2384.091490	94846.606797	59.048909
2383.803085	94653.394421	59.053914
2383.055662	94482.667881	59.058919
2382.282269	94298.134746	59.063924
2381.714187	94125.892212	59.068929
2380.885311	93946.006453	59.073933
2380.605488	93764.823869	59.078938
2379.640412	93593.675698	59.083943
2379.210333	93415.627060	59.088948
2378.636005	93232.859422	59.093953
2377.425095	93055.825247	59.098957
2376.927664	92876.643832	59.103962
2376.074630	92695.890569	59.108967
2375.682507	92519.770791	59.113972
2375.200346	92343.108675	59.118977
2374.301647	92177.154206	59.123981
2373.840242	91999.698914	59.128986
2373.090169	91818.708211	59.133991
2372.597958	91641.032410	59.138996
2372.108989	91460.948024	59.144001
2371.278710	91285.801599	59.149005
2370.886249	91096.466429	59.154010
2370.140952	90924.530473	59.159015
2369.532250	90725.753530	59.164020
2368.624462	90554.879747	59.169025
2367.538884	90362.591987	59.174029
2367.321506	90180.667990	59.179034
2366.588117	90006.987383	59.184039
2365.929179	89826.822882	59.189044
2365.411589	89645.128470	59.194049
2364.503996	89467.130355	59.199053
2364.125150	89287.851562	59.204058
2363.043772	89106.777266	59.209063
2362.342885	88926.417634	59.214068
2362.090857	88744.485743	59.219073
2361.570370	88578.466852	59.224077
2360.654117	88401.131852	59.229082
2359.791481	88228.240379	59.234087
2359.586216	88036.125208	59.239092
2359.058042	87847.378630	59.244097
2358.038857	87664.696224	59.249101
2357.707356	87473.753551	59.254106
2357.230335	87300.066621	59.259111
2356.575666	87098.515337	59.264116
2355.787716	86916.943719	59.269121
2354.752494	86731.716963	59.274125
2354.418117	86543.274387	59.279130
2353.504522	86364.504003	59.284135
2352.979199	86172.735127	59.289140
2352.162528	85994.700491	59.294145
2351.421066	85819.026252	59.299149
2350.996710	85629.369850	59.304154
2350.241552	85444.445793	59.309159
2349.826190	85263.678542	59.314164
2349.061481	85076.356719	59.319169
2348.270495	84886.961563	59.324173
2347.712889	84701.004756	59.329178
2346.956350	84522.586212	59.334183
2346.551534	84330.865501	59.339188
2345.967784	84140.765896	59.344193
2345.254617	83951.049819	59.349197
2344.648665	83769.590228	59.354202
2343.762495	83582.529044	59.359207
2343.106789	83380.803897	59.364212
2342.142712	83201.757528	59.369217
2341.550067	83026.425077	59.374221
2341.191397	82825.469446	59.379226
2340.307516	82644.361508	59.384231
2339.545154	82468.591593	59.389236
2338.750989	82277.242833	59.394241
2337.713937	82100.657580	59.399245
2337.348313	81919.638505	59.404250
2336.795532	81745.844218	59.409255
2336.513450	81562.672763	59.414260
2335.681087	81382.968229	59.419265
2334.974800	81195.437131	59.424269
2334.492529	81000.482436	59.429274
2333.302105	80823.761183	59.434279
2332.820030	80644.153239	59.439284
2332.168047	80469.402993	59.444289
2331.666005	80291.296923	59.449293
2330.866123	80094.943461	59.454298
2330.216725	79907.541705	59.459303
2329.646142	79734.521180	59.464308
2328.781258	79563.532333	59.469313
2328.247990	79378.373018	59.474317
2327.937846	79192.749054	59.479322
2326.971310	79015.754237	59.484327
2326.021755	78829.297050	59.489332
2325.637399	78644.222103	59.494337
2324.622302	78460.814062	59.499341
2324.248272	78276.355468	59.504346
2323.323180	78103.506239	59.509351
2322.975709	77913.825157	59.514356
2322.370832	77735.934885	59.519361
2321.245178	77560.669737	59.524365
2320.883304	77380.944407	59.529370
2320.156547	77202.697904	59.534375
2319.335272	77017.009912	59.539380
2319.277132	76849.071297	59.544385
2318.412470	76666.618616	59.549389
2317.708879	76478.927243	59.554394
2317.007352	76305.620568	59.559399
2316.659534	76116.501153	59.564404
2315.755212	75936.659151	59.569409
2314.879392	75768.029095	59.574413
2314.498907	75575.282990	59.579418
2313.700119	75396.221051	59.584423
2313.476270	75207.445268	59.589428
2312.657731	75020.191122	59.594433
2312.255511	74838.511549	59.599437
2311.329429	74651.689704	59.604442
2310.627550	74474.603654	59.609447
2310.059851	74278.624062	59.614452
2309.158161	74101.129492	59.619457
2308.508996	73906.078771	59.624461
2307.860414	73725.778764	59.629466
2307.219006	73542.115148	59.634471
2306.351036	73363.570081	59.639476
2306.056813	73171.441485	59.644481
2305.342723	72991.658960	59.649485
2304.836864	72796.412592	59.654490
2303.819060	72626.146242	59.659495
2303.087859	72432.307554	59.664500
2302.585523	72249.241926	59.669505
2301.665406	72069.132960	59.674509
2301.373401	71883.668077	59.679514
2300.413332	71702.852926	59.684519
2299.501017	71519.073522	59.689524
2299.015356	71337.020875	59.694529
2298.361145	71164.713953	59.699533
2298.045291	70977.899370	59.704538
2297.135663	70800.080710	59.709543
2296.476182	70625.150499	59.714548
2295.863310	70435.233586	59.719553
2294.919613	70247.809688	59.724557
2294.990550	70069.354355	59.729562
2294.380454	69882.121731	59.734567
2293.612011	69704.809962	59.739572
2292.802095	69515.344889	59.744577
2292.158104	69330.111805	59.749581
2291.737103	69132.018792	59.754586
2290.528387	68959.325047	59.759591
2290.055790	68780.669922	59.764596
2289.684424	68586.761235	59.769601
2288.580189	68405.790196	59.774605
2288.232037	68213.591641	59.779610
2287.368012	68025.549311	59.784615
2286.830766	67849.250062	59.789620
2286.142221	67665.331863	59.794625
2285.473744	67481.013212	59.799629
2285.002944	67282.174179	59.804634
2284.253823	67100.063280	59.809639
2283.624319	66911.709525	59.814644
2283.096357	66727.622736	59.819649
2282.069101	66541.982935	59.824653
2281.521161	66351.306930	59.829658
2280.586870	66160.443926	59.834663
2280.247169	65973.611258	59.839668
2279.553827	65801.402139	59.844673
2279.025346	65621.258696	59.849677
2278.625215	65422.256579	59.854682
2277.630177	65229.110467	59.859687
2276.908219	65049.664826	59.864692
2276.360750	64853.320012	59.869697
2275.369056	64677.634690	59.874701
2274.626555	64477.471312	59.879706
2274.108532	64305.893696	59.884711
2273.649182	64122.910092	59.889716
2272.855038	63940.396102	59.894721
2272.162868	63758.985319	59.899725
2271.918762	63566.712029	59.904730
2270.905158	63376.791618	59.909735
2270.286627	63186.933915	59.914740
2269.478771	63005.238382	59.919745
2268.751452	62830.876830	59.924750
2268.062801	62639.800985	59.929754
2267.423463	62449.624688	59.934759
2266.718369	62270.354458	59.939764
2265.733886	62086.371989	59.944769
2265.354154	61910.912706	59.949774
2265.028013	61737.361842	59.954778
2264.226794	61551.294591	59.959783
2263.714830	61364.993352	59.964788
2262.743161	61169.136866	59.969793
2261.990666	60992.374497	59.974798
2261.947613	60808.568557	59.979802
2260.898010	60622.720808	59.984807
2260.626173	60435.023143	59.989812
2260.144334	60244.970689	59.994817
2259.403588	60057.310019	59.999822
2258.889636	59861.562324	60.004826
2258.081969	59676.587727	60.009831
2257.391697	59486.826085	60.014836
2256.579293	59287.801731	60.019841
2255.873611	59102.034796	60.024846
2255.246142	58908.986613	60.029850
2254.545542	58730.528079	60.034855
2253.951538	58536.772587	60.039860
2253.514536	58355.686671	60.044865
2252.421198	58164.999037	60.049870
2251.847455	57966.805532	60.054874
2251.362996	57783.912759	60.059879
2250.561734	57591.817359	60.064884
2250.284621	57400.919489	60.069889
2249.602112	57209.470710	60.074894
2248.665152	57004.328282	60.079898
2247.994856	56825.630057	60.084903
2247.092406	56638.194084	60.089908
2246.433428	56447.360296	60.094913
2245.628373	56260.444414	60.099918
2245.132790	56069.462029	60.104922
2244.722671	55887.063614	60.109927
2243.949709	55694.024541	60.114932
2243.177164	55510.984770	60.119937
2242.527896	55316.097680	60.124942
2241.882928	55125.946295	60.129946
2241.135045	54941.797500	60.134951
2240.544142	54752.207886	60.139956
2239.963739	54566.707174	60.144961
2239.018979	54382.880045	60.149966
2238.873652	54196.649529	60.154970
2238.170768	54004.949400	60.159975
2237.299623	53819.559359	60.164980
2236.465575	53623.577267	60.169985
2235.850848	53437.640975	60.174990
2235.252417	53247.011306	60.179994
2234.638623	53065.920087	60.184999
2233.815126	52873.972552	60.190004
2233.307449	52683.913460	60.195009
2232.386000	52506.085159	60.200014
2232.080165	52313.191300	60.205018
2231.410559	52134.235070	60.210023
2230.573793	51943.688558	60.215028
2229.863978	51753.206187	60.220033
2229.595789	51563.256940	60.225038
2228.812693	51372.622518	60.230042
2227.964948	51179.377444	60.235047
2227.609797	50990.017549	60.240052
2227.085880	50803.375730	60.245057
2226.117889	50614.313166	60.250062
2225.795182	50425.779839	60.255066
2224.699588	50227.060279	60.260071
2224.114706	50044.735623	60.265076
2223.296368	49856.963946	60.270081
2222.721919	49667.589524	60.275086
2222.046179	49476.777891	60.280090
2221.242148	49294.837321	60.285095
2220.842738	49099.493534	60.290100
2220.226334	48902.500130	60.295105
2219.360793	48729.452044	60.300110
2218.827538	48533.287871	60.305114
2218.053719	48349.330697	60.310119
2217.316251	48156.527877	60.315124
2216.740286	47976.997284	60.320129
2215.994421	47791.307919	60.325134
2215.419045	47600.902239	60.330138
2214.563351	47414.867298	60.335143
2214.116299	47226.792452	60.340148
2213.496967	47038.044700	60.345153
2212.620494	46852.911002	60.350158
2212.169880	46667.123346	60.355162
2211.537305	46486.592002	60.360167
2210.887098	46287.811079	60.365172
2210.229988	46103.868247	60.370177
2209.346580	45919.912629	60.375182
2208.986295	45734.069885	60.380186
2208.323907	45546.274875	60.385191
2207.350444	45353.264950	60.390196
2206.874005	45156.680152	60.395201
2205.924031	44984.311603	60.400206
2205.651044	44781.138979	60.405210
2204.895597	44598.220671	60.410215
2204.395136	44418.066033	60.415220
2203.608178	44234.191898	60.420225
2202.724107	44043.203243	60.425230
2202.365023	43851.832950	60.430234
2201.454472	43676.001644	60.435239
2200.706221	43475.981035	60.440244
2200.485668	43288.317328	60.445249
2199.487075	43098.517873	60.450254
2199.202932	42918.524707	60.455258
2198.280459	42724.574417	60.460263
2197.417503	42536.634932	60.465268
2196.844411	42344.802890	60.470273
2196.370122	42161.900415	60.475278
2195.740486	41963.323644	60.480282
2194.673013	41782.404026	60.485287
2194.044967	41594.548207	60.490292
2193.780179	41403.367086	60.495297
2192.918090	41217.914670	60.500302
2192.174008	41031.655000	60.505306
2191.481224	40845.114107	60.510311
2190.875174	40663.927515	60.515316
2190.348176	40482.246503	60.520321
2189.765493	40293.768455	60.525326
2189.001715	40105.536224	60.530330
2188.232636	39912.230419	60.535335
2187.661303	39730.926451	60.540340
2187.154847	39541.252563	60.545345
2186.159544	39355.395614	60.550350
2185.673904	39160.420266	60.555354
2185.312079	38973.305026	60.560359
2184.589080	38781.410119	60.565364
2183.936837	38598.464796	60.570369
2182.823087	38416.024640	60.575374
2182.590965	38214.119600	60.580378
2181.566363	38026.509727	60.585383
2180.821911	37844.679479	60.590388
2180.370009	37659.820299	60.595393
2179.303127	37471.987742	60.600398
2178.983128	37282.107139	60.605402
2178.392426	37101.506089	60.610407
2177.757379	36911.921472	60.615412
2177.289008	36726.436509	60.620417
2176.400658	36543.511322	60.625422
2176.136306	36344.262327	60.630426
2175.326395	36164.262470	60.635431
2174.453281	35968.267834	60.640436
2174.095978	35770.620974	60.645441
2173.472918	35583.519855	60.650446
2172.910735	35386.607045	60.655450
2171.684023	35199.414733	60.660455
2171.070114	35005.963309	60.665460
2170.340089	34817.370424	60.670465
2169.228486	34646.870243	60.675470
2169.121146	34455.761360	60.680474
2168.365220	34272.716648	60.685479
2167.545088	34088.313905	60.690484
2167.030119	33898.583077	60.695489
2166.178428	33718.930638	60.700494
2165.714426	33543.144270	60.705498
2165.158361	33354.508714	60.710503
2164.355683	33166.173598	60.715508
2164.168119	32977.381136	60.720513
2163.362785	32795.578931	60.725518
2162.500253	32599.931892	60.730522
2161.719485	32423.382725	60.735527
2161.046832	32228.500080	60.740532
2160.833566	32038.704707	60.745537
2159.856522	31857.388831	60.750542
2159.193206	31663.361519	60.755546
2158.447725	31482.080976	60.760551
2158.003831	31292.740028	60.765556
2157.419158	31104.436457	60.770561
2156.470765	30922.209841	60.775566
2155.867334	30723.010787	60.780570
2155.284863	30550.119199	60.785575
2154.606816	30357.231473	60.790580
2154.211715	30167.655562	60.795585
2153.380746	29979.236474	60.800590
2152.821300	29772.729599	60.805594
2151.969210	29603.840786	60.810599
2151.401425	29411.229518	60.815604
2150.862328	29216.983873	60.820609
2149.541503	29041.657922	60.825614
2149.304052	28839.236970	60.830618
2148.526431	28653.696989	60.835623
2148.196724	28480.567557	60.840628
2147.224333	28299.239730	60.845633
2146.337537	28103.098746	60.850638
2146.365183	27910.413893	60.855642
2145.109684	27737.943214	60.860647
2144.610363	27544.657510	60.865652
2143.877934	27358.115656	60.870657
2143.075618	27166.978888	60.875662
2142.536971	26977.737721	60.880666
2141.914253	26795.402844	60.885671
2140.869403	26609.089801	60.890676
2140.202482	26438.188797	60.895681
2139.335482	26258.957793	60.900686
2138.979982	26067.530922	60.905690
2138.131694	25896.791591	60.910695
2137.825600	25726.019382	60.915700
2137.440951	25541.937535	60.920705
2136.488822	25360.641016	60.925710
2135.614681	25169.805463	60.930714
2135.353349	24996.764854	60.935719
2134.257887	24807.333453	60.940724
2133.684309	24629.892871	60.945729
2132.628624	24459.487614	60.950734
2132.507667	24274.759298	60.955738
2131.662670	24104.104849	60.960743
2130.833128	23921.902495	60.965748
2130.655708	23737.218563	60.970753
2129.493809	23563.631908	60.975758
2129.106306	23379.557980	60.980762
2128.206802	23211.012043	60.985767
2127.712107	23022.082953	60.990772
2126.871313	22855.727548	60.995777
2126.414343	22682.675908	61.000782
2125.626355	22498.115845	61.005786
2124.937282	22325.348925	61.010791
2124.249070	22144.418173	61.015796
2123.997656	21964.517752	61.020801
2123.317145	21800.639227	61.025806
2122.511251	21614.535169	61.030810
2122.127221	21432.732824	61.035815
2121.195809	21252.703609	61.040820
2120.667478	21081.089396	61.045825
2119.929229	20902.369490	61.050830
2119.553819	20706.273468	61.055834
2118.305635	20530.036585	61.060839
2117.715655	20361.980320	61.065844
2117.237680	20174.635180	61.070849
2116.627261	20004.478712	61.075854
2115.701376	19819.266770	61.080858
2115.056305	19646.706127	61.085863
2114.360895	19465.547086	61.090868
2113.618486	19293.194860	61.095873
2112.753234	19121.000206	61.100878
2112.168546	18956.206061	61.105882
2111.338710	18787.159055	61.110887
2110.713883	18607.057411	61.115892
2110.210920	18434.532569	61.120897
2109.262349	18276.285857	61.125902
2108.664652	18111.887131	61.130906
2108.074025	17944.269759	61.135911
2107.872630	17764.790727	61.140916
2107.018917	17598.895523	61.145921
2106.046940	17431.223403	61.150926
2105.292251	17262.587137	61.155930
2104.446197	17101.966354	61.160935
2103.634348	16936.956068	61.165940
2103.089125	16777.343728	61.170945
2102.167821	16618.437014	61.175950
2101.482718	16453.612055	61.180954
2100.991419	16291.565371	61.185959
2100.520386	16144.992543	61.190964
2099.933693	15979.597181	61.195969
2098.696488	15831.979714	61.200974
2098.249319	15664.241256	61.205978
2097.290508	15512.927001	61.210983
2096.649164	15358.601653	61.215988
2095.980320	15209.130962	61.220993
2094.980580	15071.187406	61.225998
2094.511153	14917.230281	61.231002
2093.814599	14774.821380	61.236007
2092.454449	14624.514610	61.241012
2091.885145	14490.866792	61.246017
2090.966654	14364.649984	61.251022
2090.384386	14225.073737	61.256026
2089.527666	14095.132758	61.261031
2088.365193	13981.079838	61.266036
2087.711930	13849.881912	61.271041
2086.501382	13741.308308	61.276046
2085.695789	13619.426172	61.281050
2085.084890	13522.646386	61.286055
2083.923898	13413.276870	61.291060
2083.087081	13318.762991	61.296065
2082.127626	13240.363193	61.301070
2081.436214	13130.829712	61.306074
2080.628074	13043.430256	61.311079
2079.663914	12971.562474	61.316084
2078.732217	12891.073413	61.321089
2077.958984	12825.056663	61.326094
2077.187319	12756.046093	61.331098
2076.215975	12681.376264	61.336103
2075.566228	12619.196307	61.341108
2074.940021	12545.063843	61.346113
2074.225892	12494.967729	61.351118
2073.497226	12425.103214	61.356122
2072.719721	12374.964484	61.361127
2072.326371	12309.896129	61.366132
2071.623395	12251.034362	61.371137
2071.117113	12192.374402	61.376142
2070.519769	12126.949175	61.381146
2069.730077	12073.466510	61.386151
2068.995933	12021.298567	61.391156
2068.491894	11958.009013	61.396161
2067.562574	11903.986466	61.401166
2067.166412	11842.579269	61.406170
2066.721253	11783.668537	61.411175
2065.944844	11723.820080	61.416180
2065.167532	11669.089110	61.421185
2064.423772	11602.209031	61.426190
2063.928280	11550.326393	61.431194
2063.267696	11499.669942	61.436199
2062.875892	11442.287243	61.441204
2062.251796	11366.298937	61.446209
2061.388271	11314.964149	61.451214
2060.932686	11252.541585	61.456218
2060.534184	11198.455860	61.461223
2059.403841	11139.678657	61.466228
2059.129440	11082.221284	61.471233
2058.204585	11030.892657	61.476238
2057.905925	10972.142328	61.481242
2056.968902	10918.052324	61.486247
2056.513791	10854.313598	61.491252
2056.024837	10786.333434	61.496257
2055.090342	10727.186675	61.501262
2054.321633	10663.261806	61.506266
2053.995460	10601.922897	61.511271
2053.154835	10542.173340	61.516276
2052.475257	10477.337580	61.521281
2051.819380	10421.508705	61.526286
2051.426783	10364.134362	61.531290
2050.767588	10309.598466	61.536295
2049.885675	10242.574121	61.541300
2049.585610	10182.865656	61.546305
2049.154110	10121.443235	61.551310
2048.209570	10057.629711	61.556314
2047.576557	9987.776845	61.561319
2046.800114	9938.758728	61.566324
2046.121771	9874.597600	61.571329
2045.454466	9815.549303	61.576334
2044.642814	9750.657940	61.581338
2043.830410	9699.390169	61.586343
2043.373536	9644.632452	61.591348
2043.050260	9581.441914	61.596353
2042.144859	9515.779031	61.601358
2041.486703	9449.762393	61.606362
2041.179716	9395.581815	61.611367
2040.341404	9329.959592	61.616372
2039.530196	9265.068677	61.621377
2038.847736	9205.333647	61.626382
2038.623630	9137.858538	61.631386
2037.789782	9086.081464	61.636391
2037.036135	9020.698441	61.641396
2036.554276	8966.409884	61.646401
2035.538338	8906.128178	61.651406
2035.024185	8848.387187	61.656410
2034.263666	8783.461514	61.661415
2034.019133	8729.486836	61.666420
2033.302777	8661.276617	61.671425
2032.646527	8605.538172	61.676430
2031.853830	8530.762099	61.681434
2030.998800	8478.710809	61.686439
2030.257299	8422.428407	61.691444
2029.839085	8350.333357	61.696449
2029.332055	8294.307310	61.701454
2028.611245	8227.894964	61.706458
2027.645544	8171.422669	61.711463
2027.050187	8110.156756	61.716468
2026.446003	8052.915540	61.721473
2025.853404	7999.954495	61.726478
2025.391307	7934.497992	61.731482
2024.507146	7880.495746	61.736487
2023.849005	7820.207390	61.741492
2023.583796	7757.053185	61.746497
2022.557187	7692.511730	61.751502
2022.187825	7623.772707	61.756506
2021.252050	7573.792043	61.761511
2020.415734	7500.975011	61.766516
2019.901098	7442.187156	61.771521
2018.982883	7385.582502	61.776526
2018.957969	7323.818275	61.781530
2018.423175	7262.528083	61.786535
2017.288125	7205.820475	61.791540
2016.717112	7142.667704	61.796545
2016.167149	7075.063489	61.801550
2015.663227	7018.153877	61.806554
2014.821499	6969.183857	61.811559
2013.968861	6903.699196	61.816564
2013.502509	6826.671084	61.821569
2012.608945	6776.438703	61.826574
2012.202282	6714.370776	61.831578
2011.248950	6647.448607	61.836583
2010.636554	6590.913609	61.841588
2010.142428	6529.795100	61.846593
2009.055233	6477.389686	61.851598
2008.572845	6415.957407	61.856602
2007.904040	6364.465705	61.861607
2007.339714	6301.223153	61.866612
2006.589303	6244.928302	61.871617
2005.786228	6199.839201	61.876622
2005.484228	6128.262185	61.881626
2004.709318	6064.205309	61.886631
2004.035745	6025.580157	61.891636
2003.180364	5959.994395	61.896641
2002.746341	5902.015449	61.901646
2002.502564	5848.863132	61.906650
2001.319438	5791.001940	61.911655
2000.602891	5727.099748	61.916660
2000.326259	5668.861674	61.921665
1999.778401	5620.625234	61.926670
1999.079163	5547.346411	61.931674
1998.431918	5486.958512	61.936679
1997.258984	5426.804163	61.941684
1996.782970	5360.769610	61.946689
1996.307047	5311.438206	61.951694
1995.443184	5250.051585	61.956698
1994.706823	5192.525671	61.961703
1993.991570	5137.317938	61.966708
1993.467551	5076.697614	61.971713
1992.608529	5034.193857	61.976718
1992.109476	4971.918358	61.981722
1991.801335	4915.933807	61.986727
1990.877771	4866.485640	61.991732
1990.133441	4801.121646	61.996737
1989.183342	4741.392191	62.001742
1989.123193	4687.519233	62.006746
1988.348982	4636.268755	62.011751
1987.464171	4578.021874	62.016756
1987.337798	4512.260570	62.021761
1986.520610	4458.182078	62.026766
1985.976586	4397.366594	62.031770
1985.292627	4331.604685	62.036775
1983.929657	4276.497462	62.041780
1983.892704	4220.530868	62.046785
1982.946458	4163.136929	62.051790
1982.351469	4105.371192	62.056794
1981.347688	4051.623517	62.061799
1980.539812	3997.831537	62.066804
1980.374216	3929.165621	62.071809
1979.422780	3890.896965	62.076814
1978.696322	3833.467061	62.081818
1978.300423	3774.587368	62.086823
1977.493754	3719.619500	62.091828
1976.969144	3661.868782	62.096833
1975.995136	3611.700161	62.101838
1975.552976	3551.853901	62.106842
1974.890835	3501.744991	62.111847
1974.172505	3456.353503	62.116852
1973.936148	3391.425405	62.121857
1972.824772	3339.327583	62.126862
1972.259129	3282.056490	62.131866
1971.945028	3228.321446	62.136871
1970.862879	3173.111494	62.141876
1970.307305	3121.795316	62.146881
1969.634944	3071.002588	62.151886
1969.278053	3007.301158	62.156890
1968.631717	2954.491301	62.161895
1967.547323	2902.101323	62.166900
1967.121513	2839.344519	62.171905
1966.083303	2796.170648	62.176910
1965.810986	2735.256611	62.181914
1964.989185	2682.759493	62.186919
1964.527132	2623.813686	62.191924
1963.768024	2567.979049	62.196929
1962.923913	2520.005625	62.201934
1962.572920	2459.242444	62.206938
1961.925761	2402.118639	62.211943
1961.078356	2354.792151	62.216948
1960.372319	2298.370494	62.221953
1959.571571	2250.806666	62.226958
1958.933660	2188.421474	62.231962
1958.224817	2133.151464	62.236967
1957.642302	2085.334305	62.241972
1957.129211	2037.682137	62.246977
1956.242320	1987.270263	62.251982
1955.750238	1926.493839	62.256986
1955.211897	1880.332672	62.261991
1954.379454	1830.348784	62.266996
1953.904786	1766.263755	62.272001
1953.315205	1721.078806	62.277006
1952.316113	1660.561400	62.282010
1951.776013	1612.724074	62.287015
1951.096360	1553.179965	62.292020
1950.419947	1504.314267	62.297025
1949.238933	1457.672922	62.302030
1948.823549	1404.772077	62.307034
1948.547822	1365.289345	62.312039
1947.504434	1316.466761	62.317044
1947.196583	1260.213803	62.322049
1946.560148	1212.516097	62.327054
1945.550623	1162.896955	62.332058
1944.929193	1114.291943	62.337063
1944.211088	1065.691401	62.342068
1943.739383	1007.147922	62.347073
1942.718309	973.812910	62.352078
1942.412332	919.725490	62.357082
1941.531218	872.553475	62.362087
1940.612358	832.093213	62.367092
1940.389754	772.609064	62.372097
1939.805944	735.601647	62.377102
1938.835570	682.211969	62.382106
1938.044467	642.671866	62.387111
1937.500431	593.408153	62.392116
1937.354862	551.215780	62.397121
1936.278941	513.176831	62.402126
1935.498437	458.846321	62.407130
1934.642847	413.581505	62.412135
1933.919893	380.515148	62.417140
1933.331839	336.893914	62.422145
1932.824255	287.898272	62.427150
1931.898148	248.538376	62.432154
1931.293568	211.272241	62.437159
1930.303260	173.846657	62.442164
1930.031404	128.561031	62.447169
1928.805197	105.170283	62.452174
1928.235405	62.581469	62.457178
1927.866124	40.270632	62.462183
1926.650955	18.258116	62.467188
1925.821957	-13.614879	62.472193
1922.389407	15.445935	62.477198
1921.075901	44.034789	62.482202
1921.147052	33.717814	62.487207
1920.759943	42.810296	62.492212
1921.014615	36.740908	62.497217
1920.665402	41.388226	62.502222
1920.015623	40.273732	62.507226
1918.940862	48.667979	62.512231
1918.035545	55.224977	62.517236
1918.046128	43.821620	62.522241
1917.214529	57.720295	62.527246
1916.134292	48.268921	62.532250
1915.387357	51.684696	62.537255
1915.406723	53.770865	62.542260
1915.129171	47.074754	62.547265
1914.203327	57.973238	62.552270
1913.423956	55.710787	62.557274
1912.595420	56.908115	62.562279
1911.534432	70.067352	62.567284
1910.842400	57.633806	62.572289
1910.431188	56.550826	62.577294
1910.241524	66.886164	62.582298
1910.034824	61.907153	62.587303
1908.955814	65.634273	62.592308
1908.372785	61.921384	62.597313
1907.479016	67.905696	62.602318
1906.245862	59.699168	62.607322
1905.898997	63.958188	62.612327
1904.797068	60.709305	62.617332
1904.867304	59.245538	62.622337
1904.564283	58.145382	62.627342
1904.136098	56.634585	62.632346
1903.282585	57.745995	62.637351
1901.820101	63.696014	62.642356
1901.836925	54.676031	62.647361
1901.175349	68.449954	62.652366
1900.467677	65.458603	62.657370
1899.777955	62.068586	62.662375
1899.093758	67.138105	62.667380
1898.340767	59.924533	62.672385
1897.574272	61.962000	62.677390
1897.021756	64.427546	62.682394
1896.517010	60.565036	62.687399
1895.469839	65.430406	62.692404
1895.405747	62.491425	62.697409
1894.553787	73.166882	62.702414
1893.779609	66.937544	62.707418
1893.100047	68.764090	62.712423
1892.485259	72.146280	62.717428
1891.609045	67.257793	62.722433
1890.826060	65.674016	62.727438
1890.246622	70.338973	62.732442
1889.552668	69.698279	62.737447
1888.724853	68.765021	62.742452
1888.348600	65.277930	62.747457
1887.984651	71.187595	62.752462
1887.480517	61.461835	62.757466
1886.707657	65.130896	62.762471
1885.495883	76.514769	62.767476
1885.024759	70.992685	62.772481
1884.905048	71.959214	62.777486
1884.175142	71.002528	62.782490
1883.452837	59.781753	62.787495
1882.326316	72.249655	62.792500
1881.907488	64.762257	62.797505
1881.126146	81.329089	62.802510
1880.529549	74.048108	62.807514
1880.047328	68.541980	62.812519
1879.104399	71.400678	62.817524
1878.772582	61.056201	62.822529
1878.178459	76.831631	62.827534
1877.368721	67.297894	62.832538
1876.950732	69.776780	62.837543
1875.968483	64.957174	62.842548
1876.050877	59.378754	62.847553
1875.275559	63.751534	62.852558
1874.596020	68.791934	62.857562
1873.693876	64.109423	62.862567
1872.239227	68.613716	62.867572
1872.418963	61.324605	62.872577
1871.299424	73.312006	62.877582
1870.200081	69.040852	62.882586
1870.505989	63.701335	62.887591
1869.662048	65.563447	62.892596
1868.881277	63.299655	62.897601
1867.792009	72.448446	62.902606
1867.196905	62.989449	62.907610
1866.610156	62.678673	62.912615
1866.603239	63.460135	62.917620
1866.029039	61.583018	62.922625
1865.213820	66.066216	62.927630
1864.507879	63.213375	62.932634
1863.944708	59.590386	62.937639
1863.193349	65.758680	62.942644
1862.517979	59.586209	62.947649
1861.049934	67.115673	62.952654
1860.464690	62.695091	62.957658
1860.690933	63.407994	62.962663
1859.706266	69.274287	62.967668
1858.721353	66.803211	62.972673
1857.926361	68.733249	62.977678
1857.396133	65.691661	62.982682
1856.686626	64.563009	62.987687
1856.377793	76.784399	62.992692
1856.056721	65.813740	62.997697
1855.213837	71.187588	63.002702
1854.313905	70.814576	63.007706
1854.120529	66.949945	63.012711
1853.376569	69.460090	63.017716
1853.021585	61.919986	63.022721
1851.681240	69.832882	63.027726
1850.803501	62.653326	63.032730
1850.106523	69.374389	63.037735
1849.394576	75.735130	63.042740
1849.006709	68.201822	63.047745
1848.157804	68.434149	63.052750
1847.901326	69.250505	63.057754
1847.535559	68.101971	63.062759
1847.062736	69.703313	63.067764
1846.673680	67.095054	63.072769
1845.513298	67.769501	63.077774
1844.222505	65.488925	63.082778
1843.622160	62.876369	63.087783
1843.068548	72.922565	63.092788
1842.818929	63.359834	63.097793
1841.810521	70.502512	63.102798
1841.321027	71.232865	63.107802
1841.184818	73.581858	63.112807
1840.010426	66.279095	63.117812
1838.918827	63.719310	63.122817
1838.259645	64.957580	63.127822
1837.425204	67.661869	63.132826
1837.447115	64.627233	63.137831
1836.615754	70.147491	63.142836
1836.166551	60.928692	63.147841
1835.489540	69.269283	63.152846
1834.988274	67.938837	63.157850
1834.619080	62.067844	63.162855
1833.494109	69.651658	63.167860
1832.551275	67.224374	63.172865
1831.758052	68.562777	63.177870
1831.183254	59.084801	63.182874
1830.736502	61.126709	63.187879
1830.048162	75.461563	63.192884
1829.780267	63.730257	63.197889
1829.471185	71.430528	63.202894
1827.815877	71.738867	63.207898
1827.169346	72.569852	63.212903
1826.171122	76.905502	63.217908
1825.714000	74.131433	63.222913
1825.005113	74.169645	63.227918
1824.851464	66.845158	63.232922
1824.403635	69.926458	63.237927
1823.633359	72.063895	63.242932
1823.453054	65.894826	63.247937
1822.374166	66.688808	63.252942
1821.081360	73.379909	63.257946
1820.928082	67.367398	63.262951
1820.098399	69.244608	63.267956
1819.842828	70.630107	63.272961
1819.052970	72.581419	63.277966
1818.390126	62.693222	63.282970
1817.521092	61.939999	63.287975
1816.239831	66.773181	63.292980
1815.975412	65.384630	63.297985
1815.184742	65.484716	63.302990
1814.760593	68.229518	63.307994
1814.607404	68.942743	63.312999
1813.846482	73.179213	63.318004
1813.838993	67.356443	63.323009
1812.579485	68.549696	63.328014
1811.279795	73.351116	63.333018
1810.820468	61.535095	63.338023
1810.020050	72.713320	63.343028
1809.980359	66.487230	63.348033
1809.709795	70.067090	63.353038
1808.180993	75.199785	63.358042
1807.505487	65.269446	63.363047
1806.703942	76.313811	63.368052
1806.429440	56.602552	63.373057
1805.562227	60.050072	63.378062
1805.157436	63.395776	63.383066
1804.577888	68.128574	63.388071
1803.564097	68.890149	63.393076
1802.852277	68.558246	63.398081
1801.908348	63.738895	63.403086
1801.186168	77.248068	63.408090
1801.167820	71.690375	63.413095
1800.566863	70.279572	63.418100
1800.356937	67.316444	63.423105
1799.716229	62.004241	63.428110
1798.636725	64.624452	63.433114
1797.570568	62.601544	63.438119
1796.837454	67.805010	63.443124
1796.598275	69.946427	63.448129
1795.969015	71.596274	63.453134
1795.784444	71.945474	63.458138
1795.037681	64.841335	63.463143
1793.596878	67.012719	63.468148
1793.440972	67.518217	63.473153
1792.521696	72.760709	63.478158
1791.338811	65.858292	63.483162
1790.453263	66.716203	63.488167
1790.468582	75.527184	63.493172
1790.110841	56.836829	63.498177
1789.287183	79.740314	63.503182
1788.616489	69.504861	63.508186
1788.266580	73.822725	63.513191
1787.127094	69.083319	63.518196
1786.186587	66.084823	63.523201
1785.319276	67.999558	63.528206
1784.785621	72.427026	63.533210
1784.567194	62.457229	63.538215
1784.113582	71.998691	63.543220
1783.982702	68.223492	63.548225
1783.585831	64.641923	63.553230
1782.401871	72.556825	63.558234
1781.547513	67.953493	63.563239
1780.692683	79.015789	63.568244
1779.857469	59.742087	63.573249
1778.590907	76.434865	63.578254
1777.970522	67.249571	63.583258
1777.905490	65.192268	63.588263
1777.200267	70.623123	63.593268
1776.774785	73.689842	63.598273
1776.365746	73.010240	63.603278
1775.925403	68.713326	63.608282
1774.805239	64.730955	63.613287
1773.674581	65.455907	63.618292
1773.128555	63.790381	63.623297
1772.604880	69.974579	63.628302
1772.197412	63.821092	63.633306
1772.146206	68.834270	63.638311
1770.990689	69.903794	63.643316
1770.008780	65.054218	63.648321
1769.445023	70.976698	63.653326
1768.872835	67.888177	63.658330
1768.629286	65.515446	63.663335
1767.255272	66.498245	63.668340
1766.406476	68.547241	63.673345
1765.858538	68.577256	63.678350
1765.276021	65.597609	63.683354
1765.030260	67.829960	63.688359
1764.488348	71.187986	63.693364
1763.838671	66.014412	63.698369
1762.744129	76.267949	63.703374
1761.852099	69.163236	63.708378
1761.367933	62.857928	63.713383
1761.077103	75.494351	63.718388
1760.701384	68.596227	63.723393
1759.237490	67.683603	63.728398
1758.642413	68.213117	63.733402
1758.192074	61.714780	63.738407
1757.550028	69.300774	63.743412
1757.411062	62.251512	63.748417
1756.232005	63.687483	63.753422
1755.100161	67.676942	63.758426
1754.733438	59.623058	63.763431
1753.879046	75.242706	63.768436
1753.681070	64.861232	63.773441
1753.048691	65.298899	63.778446
1752.456770	68.556058	63.783450
1751.838984	63.699124	63.788455
1750.726201	66.871846	63.793460
1750.314141	59.056977	63.798465
1749.399819	69.039040	63.803470
1748.993184	64.214805	63.808474
1748.863875	60.598635	63.813479
1747.460642	63.193008	63.818484
1747.125765	59.202631	63.823489
1746.176129	58.610467	63.828494
1745.461624	62.781231	63.833498
1745.653328	58.284598	63.838503
1744.110900	62.069608	63.843508
1743.205037	64.275908	63.848513
1742.449419	68.519436	63.853518
1742.111756	58.808284	63.858522
1741.940872	59.063850	63.863527
1741.332333	68.896426	63.868532
1740.974472	59.295715	63.873537
1739.886945	59.807249	63.878542
1739.026311	53.897634	63.883546
1738.703249	57.555219	63.888551
1738.107609	62.801517	63.893556
1736.779722	57.825555	63.898561
1736.114663	63.702625	63.903566
1735.604826	56.593999	63.908570
1735.286189	59.158048	63.913575
1734.780659	64.199224	63.918580
1734.080501	61.033266	63.923585
1732.792693	63.850590	63.928590
1732.141808	68.195758	63.933594
1731.647695	61.556146	63.938599
1730.863593	66.106977	63.943604
1730.655213	56.600801	63.948609
1730.025364	66.430453	63.953614
1729.315404	60.725568	63.958618
1728.522215	61.636639	63.963623
1727.554712	64.032507	63.968628
1726.918503	61.115016	63.973633
1726.593600	63.867720	63.978638
1726.117168	67.808289	63.983642
1725.806075	55.863099	63.988647
1724.319833	66.951565	63.993652
1723.913870	59.973100	63.998657
1723.148215	55.308398	64.003662
1722.716274	64.046898	64.008666
1721.824180	56.798715	64.013671
1720.699178	61.414730	64.018676
1720.373954	48.495653	64.023681
1720.063020	57.487745	64.028686
1719.412587	63.102296	64.033690
1719.147838	53.150914	64.038695
1717.802993	61.692207	64.043700
1717.314604	60.769751	64.048705
1716.482103	64.093512	64.053710
1715.869353	61.178606	64.058714
1715.622473	62.122760	64.063719
1714.675548	54.630975	64.068724
1713.555052	59.973255	64.073729
1713.266413	57.610848	64.078734
1712.475110	57.044012	64.083738
1712.276439	52.159949	64.088743
1711.817651	65.532670	64.093748
1710.782326	55.118626	64.098753
1709.945903	56.974860	64.103758
1709.441911	52.976658	64.108762
1708.945888	50.595152	64.113767
1708.004700	60.614603	64.118772
1706.953959	52.442295	64.123777
1706.305556	62.539824	64.128782
1705.860455	62.670212	64.133786
1705.382763	57.425187	64.138791
1704.726594	60.009734	64.143796
1704.326387	53.728956	64.148801
1703.618502	60.008650	64.153806
1702.595461	59.696245	64.158810
1702.427235	54.750576	64.163815
1701.742856	64.008570	64.168820
1701.203023	52.134415	64.173825
1700.033203	59.569274	64.178830
1699.277303	59.608680	64.183834
1698.783854	60.226144	64.188839
1698.450787	74.200227	64.193844
1697.669772	58.171235	64.198849
1696.669282	59.843797	64.203854
1696.057936	67.376038	64.208858
1695.878573	56.917507	64.213863
1695.367268	54.118959	64.218868
1694.198230	54.219256	64.223873
1693.292192	59.659944	64.228878
1692.338019	65.243899	64.233882
1692.412999	53.943875	64.238887
1691.657723	56.208273	64.243892
1691.256266	62.456644	64.248897
1690.240749	61.455495	64.253902
1689.350922	61.659679	64.258906
1689.001042	56.965216	64.263911
1688.398263	63.387493	64.268916
1687.840507	56.349570	64.273921
1686.757975	64.841328	64.278926
1685.847573	62.654956	64.283930
1685.797821	54.930790	64.288935
1685.064125	63.127441	64.293940
1684.945298	58.650169	64.298945
1683.505335	55.013532	64.303950
1682.764823	57.378090	64.308954
1682.269181	58.916851	64.313959
1681.849552	64.117855	64.318964
1680.859784	60.912759	64.323969
1680.055535	59.081690	64.328974
1679.425886	61.479103	64.333978
1679.368188	55.221196	64.338983
1678.895198	58.541477	64.343988
1677.950472	66.132983	64.348993
1677.104563	63.989986	64.353998
1676.664339	64.335647	64.359002
1676.124354	59.680845	64.364007
1674.619818	55.100410	64.369012
1673.933332	58.419911	64.374017
1673.255903	59.842469	64.379022
1672.925768	64.485207	64.384026
1672.699685	55.806606	64.389031
1671.959109	69.552100	64.394036
1671.298447	54.915387	64.399041
1670.467346	64.613009	64.404046
1669.507969	68.980385	64.409050
1669.496486	56.161290	64.414055
1668.314610	62.972025	64.419060
1667.680873	54.222561	64.424065
1667.267994	54.860349	64.429070
1666.463165	62.112665	64.434074
1666.259495	49.350913	64.439079
1665.244781	59.224357	64.444084
1664.436803	61.933953	64.449089
1663.984298	58.550481	64.454094
1663.348226	68.299129	64.459098
1662.631639	55.722928	64.464103
1661.580716	62.645328	64.469108
1660.946129	58.341450	64.474113
1660.678711	60.066312	64.479118
1659.918585	59.360498	64.484122
1659.499164	55.637457	64.489127
1658.272541	62.568845	64.494132
1657.583779	60.747823	64.499137
1657.409793	59.013764	64.504142
1656.634572	63.788707	64.509146
1656.424129	54.467379	64.514151
1655.054401	62.418139	64.519156
1654.528740	62.933495	64.524161
1653.934526	62.817919	64.529166
1653.616688	64.448289	64.534170
1652.563229	57.274653	64.539175
1651.207878	63.403320	64.544180
1650.976399	63.573900	64.549185
1650.935389	66.883913	64.554190
1650.304244	62.412332	64.559194
1649.884235	60.244267	64.564199
1648.420307	62.979220	64.569204
1647.921735	58.565430	64.574209
1647.376137	58.227666	64.579214
1646.692883	61.202883	64.584218
1646.237593	54.662785	64.589223
1644.781053	68.652904	64.594228
1644.526672	57.512436	64.599233
1644.190222	58.762562	64.604238
1643.703307	56.611436	64.609242
1643.227353	52.783838	64.614247
1642.075315	57.009936	64.619252
1641.613931	49.152472	64.624257
1640.888217	61.146755	64.629262
1639.937516	58.269786	64.634266
1639.313418	46.304963	64.639271
1638.448405	57.909786	64.644276
1638.086927	51.077244	64.649281
1637.995996	44.821471	64.654286
1636.687634	58.330727	64.659290
1635.788607	51.214571	64.664295
1634.866139	65.320123	64.669300
1634.608848	54.262124	64.674305
1634.309564	59.563862	64.679310
1633.887500	56.229177	64.684314
1632.953977	52.895319	64.689319
1632.292002	62.917743	64.694324
1631.790652	56.578931	64.699329
1630.853910	52.545415	64.704334
1629.835730	53.747724	64.709338
1629.560980	49.255806	64.714343
1628.732841	54.833947	64.719348
1628.579257	49.605264	64.724353
1627.524671	54.374129	64.729358
1626.458464	56.861406	64.734362
1626.432336	45.093331	64.739367
1626.104190	60.569458	64.744372
1624.964825	61.352626	64.749377
1623.901822	60.879443	64.754382
1623.380814	65.713358	64.759386
1623.122961	59.271209	64.764391
1622.516765	58.231868	64.769396
1621.377864	48.406766	64.774401
1620.703570	53.542573	64.779406
1620.195987	58.576205	64.784410
1619.897073	54.655830	64.789415
1619.083395	56.442246	64.794420
1617.982367	58.925596	64.799425
1617.445287	55.806307	64.804430
1616.845696	60.964944	64.809434
1616.673851	54.196896	64.814439
1616.018263	58.386713	64.819444
1615.093127	64.289355	64.824449
1614.428512	61.646067	64.829454
1613.697160	56.274206	64.834458
1613.410796	48.906186	64.839463
1611.832519	61.923746	64.844468
1611.213156	60.386604	64.849473
1610.742688	62.714588	64.854478
1610.625023	66.520905	64.859482
1610.390683	58.690452	64.864487
1609.004254	54.062909	64.869492
1608.348874	56.125378	64.874497
1607.789573	59.371072	64.879502
1607.329252	63.752222	64.884506
1606.277937	51.367999	64.889511
1605.249181	60.155590	64.894516
1604.990111	59.961549	64.899521
1604.583249	59.841450	64.904526
1604.034740	63.545903	64.909530
1603.392411	58.927880	64.914535
1602.249106	62.848256	64.919540
1601.593127	59.025612	64.924545
1601.458904	50.624170	64.929550
1600.344680	63.981174	64.934554
1599.736124	60.445888	64.939559
1598.949148	61.745519	64.944564
1598.439826	58.337971	64.949569
1598.349300	50.886801	64.954574
1597.479760	54.180207	64.959578
1596.707310	55.873346	64.964583
1595.871881	62.838803	64.969588
1594.999896	58.668855	64.974593
1594.316851	53.003897	64.979598
1593.360457	56.118715	64.984602
1592.871494	48.010179	64.989607
1592.434745	55.298647	64.994612
1592.369038	51.905778	64.999617
1591.532768	57.075212	65.004622
1590.156108	58.444877	65.009626
1589.882076	54.227241	65.014631
1589.622787	59.380701	65.019636
1589.104316	58.073540	65.024641
1587.921987	56.635309	65.029646
1586.769843	63.569085	65.034650
1586.567324	58.567376	65.039655
1586.114497	58.538162	65.044660
1585.491976	55.117063	65.049665
1584.798962	60.897677	65.054670
1583.671266	57.559994	65.059674
1583.641156	54.949949	65.064679
1582.430937	67.861742	65.069684
1581.684053	59.541867	65.074689
1581.172543	57.680090	65.079694
1580.792315	61.450851	65.084698
1580.593927	56.420102	65.089703
1579.243033	63.675618	65.094708
1578.413846	61.958932	65.099713
1578.035443	50.541721	65.104718
1577.372896	58.706585	65.109722
1577.088525	49.054821	65.114727
1576.001030	55.773321	65.119732
1575.179958	57.953587	65.124737
1574.763091	50.741927	65.129742
1574.236261	47.263053	65.134746
1573.268449	43.016880	65.139751
1572.266152	52.486248	65.144756
1571.792451	48.716657	65.149761
1571.692087	48.738678	65.154766
1571.268253	52.098471	65.159770
1570.258033	52.457443	65.164775
1569.392259	60.875373	65.169780
1568.909447	53.519649	65.174785
1568.567554	57.069853	65.179790
1567.448903	58.874777	65.184794
1566.738097	59.419567	65.189799
1565.818352	66.343236	65.194804
1565.754197	56.266971	65.199809
1564.608723	60.826373	65.204814
1563.532918	58.059199	65.209818
1563.168238	52.018814	65.214823
1562.779515	56.301859	65.219828
1562.708495	59.736485	65.224833
1562.098303	57.683810	65.229838
1560.799466	59.061626	65.234842
1560.673520	50.611566	65.239847
1559.624175	58.150337	65.244852
1558.425840	54.607847	65.249857
1557.756888	55.831966	65.254862
1557.308162	57.809572	65.259866
1557.016096	48.688893	65.264871
1556.261654	55.133708	65.269876
1555.473585	53.481460	65.274881
1554.938965	53.834256	65.279886
1554.491586	53.162360	65.284890
1554.200165	53.019196	65.289895
1553.081358	52.745721	65.294900
1552.067887	47.038663	65.299905
1551.685276	50.808226	65.304910
1550.692569	55.302357	65.309914
1550.558491	43.647641	65.314919
1549.528744	48.955058	65.319924
1548.639215	55.019215	65.324929
1548.545493	52.458702	65.329934
1547.870970	55.979758	65.334938
1546.872377	48.297565	65.339943
1546.010624	51.460438	65.344948
1545.706276	51.663106	65.349953
1545.159955	44.315908	65.354958
1544.222492	59.650726	65.359962
1543.416220	45.902961	65.364967
1542.578342	53.322979	65.369972
1542.231706	53.590714	65.374977
1542.055344	44.483195	65.379982
1541.325952	50.384711	65.384986
1540.789776	45.095407	65.389991
1539.487546	53.776657	65.394996
1539.466442	50.588017	65.400001
1538.492745	46.295483	65.405006
1537.230094	41.654627	65.410010
1537.105684	49.554211	65.415015
1536.671128	50.671704	65.420020
1536.016083	52.111238	65.425025
1534.676963	40.307383	65.430030
1533.969924	43.474060	65.435034
1533.579662	48.965298	65.440039
1533.196708	50.844147	65.445044
1532.853525	44.671045	65.450049
1532.197898	43.291075	65.455054
1531.373363	46.753967	65.460058
1531.067156	48.576466	65.465063
1529.905448	48.948485	65.470068
1529.020670	43.649923	65.475073
1528.541196	51.957589	65.480078
1527.830207	59.912539	65.485082
1526.985353	51.939418	65.490087
1526.074797	56.518276	65.495092
1525.640642	46.513433	65.500097
1525.328189	51.604378	65.505102
1524.805750	54.181906	65.510106
1524.296746	49.455992	65.515111
1522.976857	50.319929	65.520116
1522.278835	51.099242	65.525121
1521.909673	40.827033	65.530126
1521.436655	49.953689	65.535130
1520.564694	47.067412	65.540135
1519.681029	60.679537	65.545140
1519.443165	57.799730	65.550145
1519.092663	55.309985	65.555150
1517.583883	49.129714	65.560154
1516.840323	56.183090	65.565159
1516.214602	53.724463	65.570164
1515.712194	55.830455	65.575169
1515.900031	54.239186	65.580174
1514.825653	54.223597	65.585178
1514.085972	55.419541	65.590183
1513.445833	63.640782	65.595188
1512.994900	58.610748	65.600193
1512.130941	51.757155	65.605198
1511.205923	54.778705	65.610202
1510.638168	49.663160	65.615207
1509.997246	59.715369	65.620212
1509.316746	57.656534	65.625217
1508.656597	47.137250	65.630222
1507.759823	51.518379	65.635226
1507.697718	49.563127	65.640231
1506.485908	42.253884	65.645236
1505.586992	58.599719	65.650241
1505.081642	45.337165	65.655246
1504.797810	54.976235	65.660250
1504.470820	47.986855	65.665255
1503.830902	56.558142	65.670260
1502.999390	48.474103	65.675265
1502.289464	48.176676	65.680270
1501.135504	53.324077	65.685274
1500.318171	42.421346	65.690279
1499.743386	47.402591	65.695284
1499.114130	54.144492	65.700289
1498.731967	42.538671	65.705294
1498.287152	51.299726	65.710298
1498.123503	47.870388	65.715303
1496.771054	54.323513	65.720308
1496.079018	53.064456	65.725313
1495.652546	51.443074	65.730318
1494.739947	54.453195	65.735322
1494.127645	39.267990	65.740327
1493.286076	49.615432	65.745332
1492.891182	43.653983	65.750337
1492.581119	54.550901	65.755342
1491.423166	57.171081	65.760346
1490.964340	48.051686	65.765351
1490.290612	46.434906	65.770356
1489.649628	48.020450	65.775361
1488.726521	48.991660	65.780366
1487.510179	55.629742	65.785370
1487.196558	53.919465	65.790375
1486.826213	50.551361	65.795380
1486.472923	53.650796	65.800385
1486.030872	48.341816	65.805390
1485.363611	46.280885	65.810394
1484.837341	53.643512	65.815399
1483.841176	59.738827	65.820404
1482.787838	51.201190	65.825409
1482.261316	49.641443	65.830414
1481.831819	52.044936	65.835418
1480.950014	43.943670	65.840423
1479.877543	53.867341	65.845428
1479.386381	51.556075	65.850433
1479.451666	47.331842	65.855438
1478.421738	51.212168	65.860442
1477.407518	48.077278	65.865447
1476.761080	53.667582	65.870452
1476.671709	50.179133	65.875457
1476.028830	53.488595	65.880462
1474.717536	56.303461	65.885466
1474.078969	58.062091	65.890471
1473.747047	62.381851	65.895476
1473.404907	54.227934	65.900481
1472.538706	51.763382	65.905486
1471.501746	56.434885	65.910490
1471.070936	47.210118	65.915495
1470.462111	53.007334	65.920500
1469.459631	52.672831	65.925505
1469.102578	47.872319	65.930510
1467.997792	53.470812	65.935514
1467.984104	45.895484	65.940519
1467.406367	51.198904	65.945524
1466.158944	53.648809	65.950529
1465.551609	46.659836	65.955534
1465.112329	48.434104	65.960538
1464.760980	44.326548	65.965543
1464.196009	58.261770	65.970548
1463.012554	48.314525	65.975553
1462.650390	48.799204	65.980558
1461.791121	55.188159	65.985562
1461.232328	49.221224	65.990567
1460.000708	50.793409	65.995572
1459.758125	48.382718	66.000577
1459.492368	39.467619	66.005582
1458.491488	43.038982	66.010586
1457.697241	48.471429	66.015591
1456.778833	51.335826	66.020596
1455.990861	44.790305	66.025601
1456.090085	40.063940	66.030606
1455.639839	51.664379	66.035610
1454.947423	48.181887	66.040615
1453.851690	48.926655	66.045620
1452.861388	53.923485	66.050625
1452.909811	49.763433	66.055630
1451.852549	53.734846	66.060634
1451.261854	44.609614	66.065639
1450.690541	50.222675	66.070644
1450.324395	51.819741	66.075649
1449.133968	57.583241	66.080654
1448.511912	56.240534	66.085658
1447.936366	55.238943	66.090663
1447.062633	55.729235	66.095668
1446.289908	44.798935	66.100673
1445.848349	55.705714	66.105678
1444.880591	60.790429	66.110682
1444.773767	49.617098	66.115687
1444.486565	48.393062	66.120692
1443.595094	41.009287	66.125697
1442.807744	45.434544	66.130702
1442.159183	50.753955	66.135706
1441.193096	52.723917	66.140711
1440.541143	50.772530	66.145716
1440.314196	44.596742	66.150721
1439.742283	49.322075	66.155726
1438.746296	61.218994	66.160730
1437.644958	56.363313	66.165735
1437.506724	57.387994	66.170740
1436.722910	45.327206	66.175745
1436.088408	49.261394	66.180750
1434.855235	56.004674	66.185754
1434.758622	45.518854	66.190759
1434.144722	55.514737	66.195764
1433.842671	45.769622	66.200769
1432.735502	51.669704	66.205774
1432.043820	49.730941	66.210778
1431.423123	46.443638	66.215783
1430.910754	51.678327	66.220788
1429.759181	59.682821	66.225793
1429.354100	52.038813	66.230798
1428.520244	57.493336	66.235802
1428.395551	50.435547	66.240807
1427.526409	60.919857	66.245812
1426.550117	53.041785	66.250817
1425.936819	52.243319	66.255822
1425.217030	58.785158	66.260826
1425.394402	49.887938	66.265831
1424.060333	59.980943	66.270836
1423.281564	50.948686	66.275841
1423.165473	45.769264	66.280846
1422.508128	58.323567	66.285850
1421.716001	45.324241	66.290855
1420.701374	48.396332	66.295860
1420.119766	54.889399	66.300865
1419.987664	49.133778	66.305870
1418.573148	55.130025	66.310874
1418.151874	41.642829	66.315879
1417.625253	54.882827	66.320884
1417.234029	44.306643	66.325889
1416.581361	52.299648	66.330894
1415.136439	50.393880	66.335898
1414.911798	37.682836	66.340903
1414.256461	42.905555	66.345908
1413.552129	45.368509	66.350913
1412.818621	38.639308	66.355918
1411.908113	43.017915	66.360922
1411.906368	43.439006	66.365927
1411.098102	50.016985	66.370932
1410.062984	46.372935	66.375937
1409.379181	40.116805	66.380942
1408.791722	45.611012	66.385946
1408.341077	41.276399	66.390951
1408.166142	42.065640	66.395956
1407.092747	54.846921	66.400961
1406.751883	41.283869	66.405966
1405.517460	50.930528	66.410970
1404.485456	49.462182	66.415975
1403.717168	50.173848	66.420980
1403.165511	51.753099	66.425985
1403.136678	44.162838	66.430990
1402.237057	47.043190	66.435994
1402.241251	37.843922	66.440999
1401.413062	39.921288	66.446004
1400.846799	40.050486	66.451009
1400.439913	39.616610	66.456014
1398.738115	45.311597	66.461018
1398.437396	38.631881	66.466023
1397.452646	42.016197	66.471028
1397.074700	42.452931	66.476033
1396.458398	45.158940	66.481038
1395.570895	48.370105	66.486042
1395.337784	34.882976	66.491047
1394.735411	41.951776	66.496052
1393.952586	43.660812	66.501057
1393.103228	39.392734	66.506062
1392.545653	51.863367	66.511066
1392.042775	41.068396	66.516071
1391.090399	39.549553	66.521076
1390.089712	41.081908	66.526081
1390.193436	39.401502	66.531086
1389.144828	40.909936	66.536090
1388.143578	37.727293	66.541095
1387.673608	48.495083	66.546100
1387.072549	43.689219	66.551105
1387.034690	38.604600	66.556110
1385.835792	46.217656	66.561114
1385.107559	44.133329	66.566119
1384.423268	39.422700	66.571124
1384.043360	37.918518	66.576129
1383.422037	50.181664	66.581134
1382.269092	47.816342	66.586138
1381.507090	41.050680	66.591143
1380.992167	44.841291	66.596148
1380.575231	42.958219	66.601153
1380.537079	37.700182	66.606158
1379.157251	51.340731	66.611162
1378.721234	42.369132	66.616167
1378.386350	43.443997	66.621172
1376.778172	47.998172	66.626177
1376.168929	35.176387	66.631182
1375.342179	42.135777	66.636186
1375.484321	39.343820	66.641191
1374.898338	39.089805	66.646196
1374.633404	43.454112	66.651201
1373.931989	43.658416	66.656206
1372.662563	45.938395	66.661210
1371.789333	37.064687	66.666215
1370.972447	43.394884	66.671220
1370.081228	50.618417	66.676225
1369.650739	40.764426	66.681230
1369.208862	51.270709	66.686234
1369.387472	44.738729	66.691239
1368.194614	54.602724	66.696244
1367.493658	49.815898	66.701249
1367.196824	41.077645	66.706254
1365.635967	46.135236	66.711258
1364.944163	40.537982	66.716263
1364.305944	47.489485	66.721268
1363.659796	41.008188	66.726273
1363.816622	35.813776	66.731278
1363.101571	41.243116	66.736282
1362.319371	34.201555	66.741287
1361.825824	44.197230	66.746292
1360.738550	45.640859	66.751297
1360.003248	45.155117	66.756302
1359.110009	52.440476	66.761306
1358.921395	39.908219	66.766311
1358.333011	45.880398	66.771316
1357.282836	45.157706	66.776321
1356.796121	47.931433	66.781326
1355.774521	55.450088	66.786330
1356.002828	51.803915	66.791335
1355.086988	57.990580	66.796340
1354.012449	51.391301	66.801345
1353.825740	50.260111	66.806350
1352.989935	55.620345	66.811354
1352.351124	57.342771	66.816359
1351.574025	62.526518	66.821364
1351.178396	56.426440	66.826369
1349.936295	49.271905	66.831374
1349.084621	60.089346	66.836378
1348.701066	49.980312	66.841383
1348.402871	55.158889	66.846388
1347.796106	56.773720	66.851393
1346.647359	44.767832	66.856398
1345.844646	53.429676	66.861402
1345.401117	47.310410	66.866407
1344.935448	51.774442	66.871412
1344.469097	46.723248	66.876417
1343.591629	40.813317	66.881422
1342.576398	52.483078	66.886426
1342.201640	39.624025	66.891431
1341.944564	49.552152	66.896436
1341.255896	54.896882	66.901441
1340.125551	52.950610	66.906446
1339.524890	60.265160	66.911450
1339.193756	55.798018	66.916455
1338.362738	53.416231	66.921460
1337.383158	54.569937	66.926465
1337.411677	38.926531	66.931470
1336.762488	48.412367	66.936474
1335.736992	42.194812	66.941479
1334.808620	48.952752	66.946484
1334.220948	45.929885	66.951489
1333.870173	46.417502	66.956494
1332.571415	43.419372	66.961498
1332.080919	37.157770	66.966503
1331.449942	41.428884	66.971508
1331.156821	42.077646	66.976513
1330.849923	35.053574	66.981518
1329.766808	46.696279	66.986522
1329.250219	37.161918	66.991527
1328.633253	52.496281	66.996532
1327.542960	47.733518	67.001537
1326.622836	50.763810	67.006542
1325.644240	51.171465	67.011546
1325.429546	45.334369	67.016551
1325.242050	42.970131	67.021556
1324.819135	41.710915	67.026561
1324.575113	45.559392	67.031566
1323.253065	50.676814	67.036570
1322.870296	40.107198	67.041575
1321.963234	54.420087	67.046580
1320.721805	50.365751	67.051585
1320.737176	42.848896	67.056590
1319.385614	52.402247	67.061594
1318.742865	47.913690	67.066599
1318.100828	46.694043	67.071604
1317.569140	51.416155	67.076609
1317.523868	46.424180	67.081614
1317.000183	42.746173	67.086618
1316.293146	45.081848	67.091623
1315.242073	30.064253	67.096628
1314.396147	43.660940	67.101633
1314.252998	44.866178	67.106638
1312.966136	38.393721	67.111642
1312.469113	44.606848	67.116647
1312.097698	44.183117	67.121652
1311.180199	47.112071	67.126657
1310.375074	38.637569	67.131662
1309.549863	50.676095	67.136666
1309.381826	43.681986	67.141671
1309.071923	50.590765	67.146676
1307.917135	46.983132	67.151681
1307.289475	42.670377	67.156686
1306.453315	47.746825	67.161690
1306.401011	49.071663	67.166695
1305.593628	46.542628	67.171700
1304.429408	44.239060	67.176705
1304.211708	42.385827	67.181710
1302.916470	48.123467	67.186714
1302.194949	40.867274	67.191719
1301.590239	50.839632	67.196724
1300.898893	51.234742	67.201729
1300.898630	50.651079	67.206734
1300.091234	41.984551	67.211738
1299.721742	49.864744	67.216743
1299.028849	43.931793	67.221748
1298.312573	49.854931	67.226753
1297.435742	47.142975	67.231758
1296.489879	50.382373	67.236762
1295.981358	41.222052	67.241767
1295.546281	46.114887	67.246772
1294.704581	57.209872	67.251777
1294.249831	46.003576	67.256782
1293.594182	47.586766	67.261786
1292.634976	50.607513	67.266791
1291.740085	53.599113	67.271796
1290.628878	53.665166	67.276801
1290.994523	47.751575	67.281806
1290.019921	59.236699	67.286810
1289.851882	58.485745	67.291815
1289.009869	55.214744	67.296820
1287.952585	54.266130	67.301825
1287.815045	44.532739	67.306830
1287.010260	55.601355	67.311834
1286.140751	50.590618	67.316839
1285.243704	50.707779	67.321844
1284.713895	49.047673	67.326849
1284.301273	40.444543	67.331854
1283.334500	53.166326	67.336858
1282.588480	44.720281	67.341863
1282.387410	45.638263	67.346868
1281.676498	54.110484	67.351873
1280.887692	47.845858	67.356878
1279.761978	53.272705	67.361882
1279.524590	46.567169	67.366887
1279.274356	36.992052	67.371892
1277.856143	50.739667	67.376897
1277.519094	47.393115	67.381902
1276.333783	51.345527	67.386906
1276.471793	47.216968	67.391911
1276.156988	48.634005	67.396916
1274.720327	50.678847	67.401921
1274.250110	46.259065	67.406926
1273.810593	55.498690	67.411930
1273.369630	47.702732	67.416935
1272.141164	47.615550	67.421940
1271.347167	48.678271	67.426945
1271.023553	46.712571	67.431950
1270.152653	43.960259	67.436954
1269.584874	46.568694	67.441959
1268.852859	44.309963	67.446964
1268.554665	40.435265	67.451969
1267.868947	38.134481	67.456974
1266.429648	42.444247	67.461978
1266.359601	41.518442	67.466983
1265.811634	40.186081	67.471988
1265.330521	41.154900	67.476993
1264.504599	37.301036	67.481998
1263.928157	52.450764	67.487002
1263.290873	42.550835	67.492007
1262.092739	45.024534	67.497012
1261.067739	55.016418	67.502017
1261.218963	43.250159	67.507022
1260.675521	45.017365	67.512026
1260.008259	39.001506	67.517031
1259.017574	39.824269	67.522036
1258.165258	44.384481	67.527041
1258.033852	45.873284	67.532046
1256.889338	52.149951	67.537050
1255.690001	37.920779	67.542055
1255.427166	36.339656	67.547060
1254.943172	47.931275	67.552065
1254.919027	34.530801	67.557070
1254.334607	38.876528	67.562074
1253.276749	45.398035	67.567079
1252.711204	37.282854	67.572084
1251.565169	51.512326	67.577089
1250.649202	43.418169	67.582094
1249.930232	38.292051	67.587098
1249.611438	42.122458	67.592103
1249.278632	46.097021	67.597108
1248.800827	48.342647	67.602113
1248.063022	41.376068	67.607118
1246.883045	46.928248	67.612122
1246.989584	45.781977	67.617127
1246.120788	46.892869	67.622132
1244.883728	53.368760	67.627137
1244.457266	32.423473	67.632142
1243.828076	40.786504	67.637146
1243.509154	37.389770	67.642151
1242.457961	43.240016	67.647156
1241.660199	52.123445	67.652161
1241.429566	44.585788	67.657166
1240.793612	40.890959	67.662170
1240.013441	42.363075	67.667175
1239.284693	36.629813	67.672180
1238.458453	45.896235	67.677185
1238.215015	37.302486	67.682190
1237.019493	44.826751	67.687194
1236.324535	43.736966	67.692199
1236.162340	41.051746	67.697204
1235.427499	36.517937	67.702209
1234.821520	41.403259	67.707214
1233.698370	42.266019	67.712218
1233.486012	41.788622	67.717223
1232.771646	38.503656	67.722228
1231.670781	37.254491	67.727233
1231.480334	30.871088	67.732238
1230.665933	42.114698	67.737242
1230.216319	45.153781	67.742247
1229.161482	41.172327	67.747252
1227.926703	45.039584	67.752257
1227.959830	40.374195	67.757262
1227.020875	48.122595	67.762266
1227.029881	41.556085	67.767271
1226.091596	42.097715	67.772276
1225.238553	48.682858	67.777281
1224.855906	34.620308	67.782286
1224.392971	42.368704	67.787290
1223.365506	36.049015	67.792295
1222.774036	39.493854	67.797300
1221.855951	42.339352	67.802305
1221.661716	31.793405	67.807310
1220.584468	51.324690	67.812314
1220.087589	46.652117	67.817319
1219.640005	41.705203	67.822324
1218.832751	44.085224	67.827329
1218.388098	48.965398	67.832334
1217.381117	47.023220	67.837338
1216.965667	48.590309	67.842343
1215.936693	44.641017	67.847348
1214.993615	46.356665	67.852353
1214.851704	43.360716	67.857358
1214.031803	45.100931	67.862362
1213.990785	43.016184	67.867367
1213.103153	40.733332	67.872372
1212.031624	48.599013	67.877377
1211.680207	42.460402	67.882382
1210.513370	43.451544	67.887386
1209.854774	39.553745	67.892391
1209.243523	40.193185	67.897396
1208.834646	47.340056	67.902401
1208.692865	46.015653	67.907406
1207.525479	48.497102	67.912410
1206.999577	48.186263	67.917415
1206.563926	40.104054	67.922420
1205.859500	43.669362	67.927425
1204.592655	35.050711	67.932430
1204.155736	43.783719	67.937434
1203.596941	43.727269	67.942439
1203.308696	41.732301	67.947444
1202.191680	44.227819	67.952449
1201.911390	40.105858	67.957454
1200.985369	40.921513	67.962458
1200.206603	41.221743	67.967463
1199.455461	40.595065	67.972468
1198.481025	49.071359	67.977473
1197.950062	37.880373	67.982478
1197.652718	41.010361	67.987482
1197.181368	38.082575	67.992487
1196.171371	40.942697	67.997492
1195.435334	39.782186	68.002497
1194.937891	37.960837	68.007502
1194.761816	45.838659	68.012506
1193.768991	43.787008	68.017511
1193.025264	57.397437	68.022516
1192.069306	56.544713	68.027521
1191.916356	45.509649	68.032526
1190.439221	48.194906	68.037530
1189.706621	41.874070	68.042535
1189.494581	45.356346	68.047540
1188.891029	41.905537	68.052545
1189.070168	47.246329	68.057550
1187.965704	51.354654	68.062554
1187.321807	48.287151	68.067559
1186.590535	41.838372	68.072564
1185.862620	52.628275	68.077569
1185.291759	44.927117	68.082574
1184.124610	53.544452	68.087578
1183.595468	46.497401	68.092583
1183.164504	44.446285	68.097588
1181.849382	49.775557	68.102593
1181.765063	37.680915	68.107598
1181.105976	48.373138	68.112602
1180.714022	49.220560	68.117607
1179.926311	40.927843	68.122612
1179.085528	41.763066	68.127617
1178.723190	39.901311	68.132622
1177.995378	46.876555	68.137626
1177.009282	38.530236	68.142631
1176.570223	43.196636	68.147636
1176.113131	47.910060	68.152641
1175.580301	35.339548	68.157646
1174.265308	50.499504	68.162650
1173.632842	53.764796	68.167655
1173.222514	42.810095	68.172660
1172.419089	51.573013	68.177665
1171.507502	45.074067	68.182670
1170.868377	46.670428	68.187674
1170.607647	44.622202	68.192679
1170.392680	39.564188	68.197684
1169.227821	44.281365	68.202689
1168.521710	37.048003	68.207694
1167.687546	47.794879	68.212698
1167.308253	43.154082	68.217703
1166.972038	43.909063	68.222708
1165.812152	46.094447	68.227713
1165.214236	42.939214	68.232718
1164.567963	46.730249	68.237722
1164.215080	39.278284	68.242727
1163.305411	42.974015	68.247732
1162.348770	51.523184	68.252737
1162.038451	41.574445	68.257742
1161.614983	49.961546	68.262746
1160.667947	50.173432	68.267751
1159.998538	43.803132	68.272756
1159.666932	43.800445	68.277761
1158.795559	37.244650	68.282766
1157.733668	44.772924	68.287770
1157.357354	44.337379	68.292775
1157.008666	40.475461	68.297780
1155.594146	44.924845	68.302785
1155.430060	29.752081	68.307790
1154.431667	39.660906	68.312794
1154.391996	36.803244	68.317799
1153.561977	40.778045	68.322804
1152.340902	41.632760	68.327809
1152.014555	33.689303	68.332814
1151.484096	43.700327	68.337818
1150.620085	39.702752	68.342823
1149.826032	46.237530	68.347828
1149.343505	45.617030	68.352833
1148.771674	44.572341	68.357838
1148.353706	49.645399	68.362842
1147.729567	37.371692	68.367847
1147.066857	49.456942	68.372852
1146.317629	45.745462	68.377857
1145.259108	41.494974	68.382862
1144.181238	46.122632	68.387866
1143.691456	41.027906	68.392871
1143.661825	42.795414	68.397876
1143.218195	48.966956	68.402881
1142.308621	40.330938	68.407886
1141.288940	45.452389	68.412890
1141.011719	43.684333	68.417895
1140.573885	39.227895	68.422900
1139.247986	44.142585	68.427905
1138.920124	43.500641	68.432910
1138.228813	45.064308	68.437914
1137.666081	41.458787	68.442919
1136.873963	37.736788	68.447924
1135.894504	51.386291	68.452929
1135.656073	30.524683	68.457934
1135.216571	42.875624	68.462938
1134.205124	41.796783	68.467943
1133.430921	40.088852	68.472948
1132.978403	44.282736	68.477953
1132.686646	41.014162	68.482958
1131.412140	45.639984	68.487962
1130.889578	43.802143	68.492967
1130.630607	31.766832	68.497972
1129.587318	40.563174	68.502977
1128.716311	39.936659	68.507982
1128.132765	41.278185	68.512986
1127.883337	41.439049	68.517991
1127.139221	42.533303	68.522996
1125.772531	46.238660	68.528001
1125.454059	40.712992	68.533006
1124.642224	55.196853	68.538010
1124.148596	43.022240	68.543015
1124.186593	43.957401	68.548020
1122.928495	51.105314	68.553025
1122.479895	48.173922	68.558030
1121.919606	47.160520	68.563034
1120.773738	43.548408	68.568039
1119.747784	49.738459	68.573044
1119.268433	44.463884	68.578049
1119.071624	42.378690	68.583054
1118.733810	48.833023	68.588058
1118.153236	48.213931	68.593063
1117.384407	42.835591	68.598068
1116.526717	48.793876	68.603073
1115.851944	37.862333	68.608078
1114.773577	43.587636	68.613082
1114.113369	42.202200	68.618087
1113.816012	47.480003	68.623092
1113.298961	54.123697	68.628097
1112.100847	45.511508	68.633102
1111.593904	50.480451	68.638106
1111.354794	40.629207	68.643111
1110.894472	43.124386	68.648116
1109.800123	43.999964	68.653121
1109.196251	33.506580	68.658126
1108.387585	44.571108	68.663130
1108.027188	37.571359	68.668135
1107.329203	37.707380	68.673140
1106.340454	44.679990	68.678145
1106.176891	39.960737	68.683150
1104.758330	39.544328	68.688154
1103.858238	40.471010	68.693159
1103.510395	36.771394	68.698164
1102.823559	38.638709	68.703169
1102.738952	32.016140	68.708174
1102.197502	43.471824	68.713178
1101.551171	34.163176	68.718183
1100.825951	37.821701	68.723188
1100.017132	39.277913	68.728193
1099.094353	35.592481	68.733198
1098.354578	32.202791	68.738202
1097.756825	35.437342	68.743207
1097.679977	36.270922	68.748212
1096.168246	40.850915	68.753217
1095.708928	32.608502	68.758222
1094.786895	39.606770	68.763226
1094.364823	37.511680	68.768231
1094.566964	40.027639	68.773236
1093.508636	42.900218	68.778241
1092.847063	38.160838	68.783246
1092.151446	32.967983	68.788250
1091.587253	35.577456	68.793255
1090.610291	39.728612	68.798260
1089.789852	38.438057	68.803265
1089.786858	32.076895	68.808270
1088.579980	40.769963	68.813274
1087.956504	38.437253	68.818279
1087.423791	34.264002	68.823284
1086.888806	42.828115	68.828289
1085.944459	31.067419	68.833294
1085.052725	41.197418	68.838298
1084.556266	40.344181	68.843303
1084.000847	37.759374	68.848308
1083.341082	37.165504	68.853313
1082.879235	34.677776	68.858318
1081.962638	41.003405	68.863322
1081.453045	43.339269	68.868327
1081.035041	38.239449	68.873332
1079.845616	47.241983	68.878337
1079.355647	36.583832	68.883342
1078.835156	43.057763	68.888346
1078.072933	37.914930	68.893351
1077.098175	37.013201	68.898356
1076.430560	40.927496	68.903361
1076.370710	37.705619	68.908366
1075.638622	46.392553	68.913370
1074.756128	38.906585	68.918375
1074.133120	38.437756	68.923380
1073.568888	39.978070	68.928385
1073.192864	23.962262	68.933390
1071.810843	38.073196	68.938394
1071.230826	34.431020	68.943399
1071.109529	40.068744	68.948404
1070.254823	44.414925	68.953409
1069.736396	40.379753	68.958414
1068.850719	43.967618	68.963418
1068.183781	44.439332	68.968423
1067.633090	36.649851	68.973428
1066.279193	40.443087	68.978433
1066.285884	39.230694	68.983438
1065.601542	47.507913	68.988442
1065.164340	39.359757	68.993447
1064.037481	36.771242	68.998452
1063.185985	40.656445	69.003457
1062.917281	39.227666	69.008462
1062.254157	54.405390	69.013466
1061.794037	35.780485	69.018471
1061.077039	29.772608	69.023476
1060.022657	41.300430	69.028481
1059.924999	34.672056	69.033486
1058.754499	43.766201	69.038490
1057.883867	40.149759	69.043495
1057.598979	36.624639	69.048500
1056.986970	44.382574	69.053505
1056.781318	31.056741	69.058510
1055.449288	35.324317	69.063514
1054.929076	40.271722	69.068519
1054.723768	37.577608	69.073524
1053.261376	44.294425	69.078529
1052.612345	39.426905	69.083534
1052.320532	38.977933	69.088538
1051.612748	38.904218	69.093543
1051.556984	40.035642	69.098548
1050.259058	41.016171	69.103553
1049.961698	32.877314	69.108558
1049.247036	38.287736	69.113562
1048.040049	45.821783	69.118567
1047.775698	33.508227	69.123572
1046.946072	46.522054	69.128577
1046.896999	39.996336	69.133582
1045.633813	39.810707	69.138586
1045.313362	38.185160	69.143591
1044.587797	40.333039	69.148596
1043.399759	45.228995	69.153601
1042.907344	35.377066	69.158606
1041.978533	45.126625	69.163610
1041.301795	43.302293	69.168615
1041.116313	39.088004	69.173620
1041.088255	36.023496	69.178625
1040.064619	32.781486	69.183630
1039.137215	41.665076	69.188634
1038.518138	46.011627	69.193639
1037.642535	42.689295	69.198644
1036.807121	43.507940	69.203649
1036.477597	38.938100	69.208654
1035.995031	34.020450	69.213658
1035.297609	45.620803	69.218663
1034.400203	42.541637	69.223668
1033.868056	41.541125	69.228673
1033.587343	37.338834	69.233678
1032.439771	33.085222	69.238682
1031.814373	37.145773	69.243687
1031.313065	37.116485	69.248692
1030.680004	39.790543	69.253697
1029.808840	38.487578	69.258702
1028.926351	41.347976	69.263706
1028.314631	50.096195	69.268711
1028.537125	40.203068	69.273716
1027.021086	43.165838	69.278721
1026.171526	40.126372	69.283726
1026.002311	50.308598	69.288730
1025.743690	50.433089	69.293735
1024.732618	45.664175	69.298740
1023.625271	49.309400	69.303745
1023.459491	40.048902	69.308750
1022.576029	48.159113	69.313754
1021.270144	43.654724	69.318759
1021.187574	42.073334	69.323764
1020.687635	54.889643	69.328769
1020.494469	44.403480	69.333774
1019.468465	46.837285	69.338778
1018.768684	37.988175	69.343783
1017.979472	37.090066	69.348788
1017.243727	51.162866	69.353793
1016.981516	37.555877	69.358798
1015.818058	51.389222	69.363802
1015.196001	54.216077	69.368807
1015.008545	49.950063	69.373812
1013.476612	53.691229	69.378817
1013.038174	39.617115	69.383822
1012.713682	51.039871	69.388826
1012.381229	52.853981	69.393831
1011.638760	46.202041	69.398836
1010.545022	49.198558	69.403841
1009.859017	49.266468	69.408846
1009.569603	52.131863	69.413850
1008.628516	49.859167	69.418855
1008.224705	43.404083	69.423860
1007.546170	45.792070	69.428865
1007.150028	32.055010	69.433870
1005.810842	46.652747	69.438874
1004.955867	45.205288	69.443879
1004.804646	46.735098	69.448884
1004.367106	54.252401	69.453889
1003.841773	40.006034	69.458894
1002.854609	46.931117	69.463898
1001.994510	48.941142	69.468903
1001.875529	48.062556	69.473908
1000.177313	49.507343	69.478913
1000.006253	39.623218	69.483918
999.414984	45.438219	69.488922
998.867811	45.739509	69.493927
998.718671	44.744297	69.498932
997.382949	43.072135	69.503937
996.757083	44.984969	69.508942
996.202045	49.788116	69.513946
995.762221	46.568351	69.518951
994.622668	49.833937	69.523956
993.735163	50.108953	69.528961
993.704661	40.240311	69.533966
993.295327	42.219618	69.538970
992.043696	50.653345	69.543975
991.362241	37.775384	69.548980
990.713548	43.361404	69.553985
990.614026	43.968361	69.558990
989.098005	43.201672	69.563994
988.509811	51.857846	69.568999
988.369789	50.066402	69.574004
987.628620	49.688935	69.579009
987.577194	43.666641	69.584014
986.601967	45.062633	69.589018
985.706380	43.422948	69.594023
985.165449	47.348647	69.599028
983.814817	48.036399	69.604033
983.549746	40.100571	69.609038
982.857615	48.415314	69.614042
982.653258	41.346608	69.619047
981.523490	48.521468	69.624052
980.369495	52.182018	69.629057
980.035612	45.755236	69.634062
979.522940	47.754142	69.639066
979.378449	48.413986	69.644071
978.915945	38.782818	69.649076
977.604868	44.630353	69.654081
977.300822	41.291218	69.659086
976.318097	44.252737	69.664090
975.487006	49.607588	69.669095
974.688511	45.199110	69.674100
974.215496	45.945920	69.679105
974.057603	37.207723	69.684110
973.029102	51.375997	69.689114
971.919041	46.143466	69.694119
971.704343	41.151668	69.699124
971.056732	53.903166	69.704129
971.007668	43.073964	69.709134
969.669192	45.363543	69.714138
969.132654	44.584516	69.719143
968.848925	42.677170	69.724148
967.545473	45.781189	69.729153
966.878787	41.042660	69.734158
966.268320	46.449140	69.739162
965.866007	41.007804	69.744167
965.633228	45.475828	69.749172
964.369229	37.128099	69.754177
964.073502	36.703415	69.759182
963.351138	38.980116	69.764186
962.238145	43.878357	69.769191
961.613663	33.413536	69.774196
960.904642	43.345759	69.779201
961.041552	39.792960	69.784206
960.179004	41.576307	69.789210
958.733513	42.768019	69.794215
958.733630	46.557167	69.799220
957.976609	41.968632	69.804225
957.383516	39.678432	69.809230
956.519206	33.025405	69.814234
956.220949	40.791776	69.819239
955.455047	36.682472	69.824244
954.084243	44.857631	69.829249
953.437123	33.470748	69.834254
953.180144	44.310325	69.839258
952.819158	43.153285	69.844263
952.380867	35.964116	69.849268
951.149444	42.191647	69.854273
950.853208	41.342847	69.859278
950.198963	40.156779	69.864282
948.971667	43.874735	69.869287
948.497275	35.700990	69.874292
947.657577	45.067388	69.879297
947.553083	28.497478	69.884302
946.710598	39.619455	69.889306
945.577860	42.456622	69.894311
945.627035	37.514303	69.899316
944.720739	44.461227	69.904321
944.335916	39.228424	69.909326
943.047057	43.471840	69.914330
942.577161	39.657634	69.919335
942.278288	30.454604	69.924340
941.381915	34.775910	69.929345
940.764435	29.318362	69.934350
940.050897	36.972620	69.939354
939.529130	42.456451	69.944359
938.421620	33.768449	69.949364
937.416258	28.129776	69.954369
937.185397	30.381885	69.959374
936.753949	40.129593	69.964378
936.358245	41.515384	69.969383
936.079749	36.734017	69.974388
934.551802	41.332449	69.979393
934.259420	27.891139	69.984398
933.647356	27.272372	69.989402
932.542105	28.230183	69.994407
931.974223	36.794814	69.999412
931.251952	41.659274	70.004417
930.947605	32.744120	70.009422
929.992498	28.396856	70.014426
929.098382	34.988606	70.019431
929.026038	32.847356	70.024436
928.422140	38.454643	70.029441
927.987047	33.346540	70.034446
926.676853	34.876282	70.039450
925.988414	35.551726	70.044455
925.940523	32.872000	70.049460
924.676732	34.665594	70.054465
924.062057	28.784983	70.059470
923.218502	35.556345	70.064474
923.045306	35.244630	70.069479
922.628525	30.261348	70.074484
921.440345	39.437201	70.079489
920.627302	34.034432	70.084494
920.581923	33.738646	70.089498
919.501514	40.530358	70.094503
918.862377	34.622100	70.099508
918.345718	31.249003	70.104513
917.689178	33.155696	70.109518
916.559434	37.387994	70.114522
916.136201	39.115636	70.119527
915.448128	33.128435	70.124532
915.171036	43.608515	70.129537
914.882838	31.317711	70.134542
913.974331	33.256618	70.139546
913.245547	33.282477	70.144551
912.258153	35.967219	70.149556
910.934065	43.308643	70.154561
910.760535	31.152556	70.159566
910.209738	39.332852	70.164570
909.870199	38.643912	70.169575
909.361480	30.097178	70.174580
908.258336	33.726006	70.179585
908.107517	32.950264	70.184590
906.910056	37.196496	70.189594
905.916557	36.207932	70.194599
905.329894	29.465012	70.199604
904.890906	30.368843	70.204609
905.081280	29.868383	70.209614
903.700235	41.944974	70.214618
902.865390	47.462867	70.219623
902.700812	40.320035	70.224628
901.820170	44.705085	70.229633
900.960998	35.748923	70.234638
900.329624	42.339871	70.239642
899.677264	42.374072	70.244647
899.257233	36.853571	70.249652
897.893361	38.465987	70.254657
897.454033	33.733877	70.259662
897.204003	35.433956	70.264666
896.559708	41.831420	70.269671
896.293005	36.627139	70.274676
894.985963	38.169011	70.279681
894.413859	37.897129	70.284686
894.056553	33.872630	70.289690
892.770232	36.221754	70.294695
892.006529	31.793581	70.299700
891.289402	39.699155	70.304705
891.340418	31.940125	70.309710
890.796745	35.009992	70.314714
890.349312	37.645077	70.319719
889.648635	31.773432	70.324724
888.676787	38.380720	70.329729
887.763989	33.473231	70.334734
886.856450	32.980347	70.339738
886.168995	33.084792	70.344743
885.950782	36.098133	70.349748
885.383302	42.486528	70.354753
884.557946	38.123360	70.359758
883.664148	29.215298	70.364762
883.507887	32.393820	70.369767
883.177848	24.834210	70.374772
881.609167	37.606139	70.379777
881.330689	33.584865	70.384782
880.553904	38.558937	70.389786
879.972281	36.098199	70.394791
879.069525	25.343390	70.399796
878.091723	37.991318	70.404801
878.009135	27.907063	70.409806
877.341639	37.425836	70.414810
877.160020	36.975117	70.419815
876.545796	28.878844	70.424820
875.751493	35.074680	70.429825
874.665846	31.159797	70.434830
873.976023	38.655754	70.439834
873.369132	35.554069	70.444839
872.973600	31.387425	70.449844
871.631261	39.737860	70.454849
871.065278	29.719500	70.459854
870.770116	29.360970	70.464858
870.044828	34.334731	70.469863
869.267539	27.179041	70.474868
868.229921	33.453028	70.479873
867.766076	28.901446	70.484878
867.600859	33.924839	70.489882
867.206101	39.126692	70.494887
866.355169	32.859502	70.499892
865.332647	44.128424	70.504897
865.069972	34.150099	70.509902
863.625573	40.769528	70.514906
862.977885	37.081408	70.519911
862.767072	36.359372	70.524916
862.247357	43.503409	70.529921
861.928754	42.817451	70.534926
860.824994	42.390500	70.539930
860.038765	38.344387	70.544935
859.880873	37.850470	70.549940
858.175673	42.019842	70.554945
857.624767	31.508657	70.559950
857.212795	33.765943	70.564954
856.538242	32.483787	70.569959
856.763282	31.927344	70.574964
855.899803	37.967041	70.579969
855.068446	31.217350	70.584974
854.132386	29.735544	70.589978
853.484078	38.186832	70.594983
852.744215	32.603709	70.599988
851.896544	39.468786	70.604993
851.497367	34.735026	70.609998
851.165974	31.199994	70.615002
850.322194	34.040094	70.620007
849.608932	30.231530	70.625012
848.754281	43.372376	70.630017
848.372307	36.089114	70.635022
847.695214	32.536567	70.640026
846.735142	37.828400	70.645031
846.553684	24.825197	70.650036
845.715011	36.667248	70.655041
844.849513	34.738978	70.660046
844.317601	38.820957	70.665050
843.613908	39.115654	70.670055
843.486594	31.897517	70.675060
842.040832	31.649588	70.680065
841.491531	37.358586	70.685070
841.126522	39.032817	70.690074
839.933045	37.508410	70.695079
839.456386	26.545450	70.700084
838.610536	36.958359	70.705089
838.191922	31.432918	70.710094
838.192607	34.354649	70.715098
836.967984	30.589636	70.720103
836.300509	26.773791	70.725108
835.697290	42.478148	70.730113
835.257284	31.657584	70.735118
834.485938	32.492904	70.740122
833.704226	35.438246	70.745127
833.296144	39.949946	70.750132
832.580219	45.877857	70.755137
831.762613	33.348065	70.760142
831.037508	39.592824	70.765146
830.385354	41.050989	70.770151
830.026749	33.683589	70.775156
828.415354	36.034025	70.780161
828.058609	33.895472	70.785166
827.780561	29.388442	70.790170
827.309450	33.580592	70.795175
826.678729	24.851456	70.800180
825.879681	42.383121	70.805185
825.273079	33.601256	70.810190
824.496473	34.454762	70.815194
823.452747	30.708271	70.820199
822.977212	33.589110	70.825204
822.145564	41.804662	70.830209
821.731199	34.864029	70.835214
821.656768	39.064003	70.840218
820.080020	36.059940	70.845223
819.768326	34.945538	70.850228
818.967018	50.396009	70.855233
818.730112	37.991404	70.860238
818.109738	44.561693	70.865242
817.057895	40.203063	70.870247
816.689932	32.230034	70.875252
816.138314	39.746580	70.880257
815.199183	33.428796	70.885262
814.454923	32.968295	70.890266
813.717200	34.356506	70.895271
813.883630	30.989818	70.900276
812.325842	29.688995	70.905281
811.770521	39.134731	70.910286
811.361371	41.651771	70.915290
810.151055	39.450397	70.920295
809.546235	37.349758	70.925300
808.793172	32.344337	70.930305
808.581432	38.717115	70.935310
808.384185	37.969270	70.940314
807.309433	35.049310	70.945319
806.929742	29.429372	70.950324
805.892182	39.418647	70.955329
805.676770	34.051677	70.960334
804.330545	38.774216	70.965338
803.499965	37.505872	70.970343
803.120652	34.420019	70.975348
802.784045	42.055306	70.980353
802.582852	31.843283	70.985358
801.496066	39.189557	70.990362
800.769202	42.157717	70.995367
800.529211	38.187099	71.000372
799.197061	40.825837	71.005377
798.667320	38.175512	71.010382
798.034562	40.154142	71.015386
797.636584	38.170390	71.020391
796.755541	26.254688	71.025396
795.794494	39.746788	71.030401
795.554564	33.841254	71.035406
795.099915	28.094480	71.040410
793.696675	37.142188	71.045415
793.165595	24.189922	71.050420
792.574976	34.068627	71.055425
792.334748	31.714415	71.060430
791.479822	38.389852	71.065434
790.748479	36.479669	71.070439
790.656026	36.483114	71.075444
789.683237	42.483462	71.080449
788.866076	33.381892	71.085454
788.396978	34.107611	71.090458
787.140251	32.681608	71.095463
786.336194	26.619878	71.100468
785.451234	41.769851	71.105473
784.816307	34.145253	71.110478
784.725807	31.812938	71.115482
784.460959	34.638167	71.120487
784.361619	28.391714	71.125492
783.347598	33.881387	71.130497
782.432208	41.388040	71.135502
781.475127	32.330826	71.140506
780.254731	37.148462	71.145511
780.052193	32.116912	71.150516
779.683699	44.262599	71.155521
779.162482	38.703040	71.160526
778.425218	44.009890	71.165530
777.487075	50.189231	71.170535
777.148285	31.554590	71.175540
776.368361	46.503346	71.180545
775.473524	43.953724	71.185550
774.691866	33.110296	71.190554
774.103650	41.321798	71.195559
773.881803	39.600168	71.200564
772.750982	42.310948	71.205569
772.126679	42.785413	71.210574
771.648890	38.841616	71.215578
771.160114	41.656764	71.220583
770.371286	45.423268	71.225588
769.519805	44.613999	71.230593
768.847778	37.069428	71.235598
768.711656	43.305592	71.240602
767.220397	43.348798	71.245607
766.851719	40.373221	71.250612
766.200449	38.481837	71.255617
765.767672	38.684540	71.260622
765.575292	37.453380	71.265626
764.120579	40.274072	71.270631
763.743849	34.059164	71.275636
763.207139	37.851763	71.280641
762.023848	37.377593	71.285646
761.134207	39.458628	71.290650
760.491627	39.893427	71.295655
760.435132	37.978319	71.300660
760.172617	30.542023	71.305665
759.216978	40.551387	71.310670
758.604600	42.209817	71.315674
757.832282	36.521507	71.320679
757.551905	27.108996	71.325684
755.857472	38.525914	71.330689
755.542119	30.817335	71.335694
755.081427	33.194355	71.340698
754.908084	40.843075	71.345703
754.067656	32.702429	71.350708
752.936135	39.812993	71.355713
752.641408	39.180019	71.360718
752.055291	31.375777	71.365722
751.053939	35.336966	71.370727
750.529571	32.245832	71.375732
749.832132	39.244712	71.380737
749.289058	44.109071	71.385742
748.729589	40.446363	71.390746
747.768332	43.639510	71.395751
747.424719	37.990184	71.400756
745.805879	35.792381	71.405761
745.482785	34.905306	71.410766
745.048793	38.282589	71.415770
744.671483	41.679234	71.420775
744.418535	30.917225	71.425780
743.408100	40.690891	71.430785
742.215199	37.734578	71.435790
742.001518	31.752335	71.440794
741.180280	31.734616	71.445799
740.413604	29.390109	71.450804
739.624490	36.947629	71.455809
739.440530	35.374512	71.460814
739.109624	35.841697	71.465818
737.668350	42.826543	71.470823
737.375660	39.156057	71.475828
736.865223	40.374065	71.480833
736.009586	40.615711	71.485838
735.185820	37.069203	71.490842
734.202980	40.975414	71.495847
733.984128	42.228999	71.500852
733.443341	43.723073	71.505857
732.296754	39.314913	71.510862
731.367307	39.593544	71.515866
730.988697	40.691217	71.520871
730.609561	36.406873	71.525876
730.616574	37.151416	71.530881
729.755230	36.832583	71.535886
729.048032	43.329979	71.540890
728.048722	48.777911	71.545895
727.568750	45.905213	71.550900
726.432265	46.038615	71.555905
726.039863	32.215892	71.560910
725.541096	39.913269	71.565914
724.571503	39.299438	71.570919
723.755761	34.203101	71.575924
723.398061	38.252632	71.580929
722.862719	31.559942	71.585934
722.342062	35.368915	71.590938
721.460426	34.980776	71.595943
721.239327	31.637939	71.600948
719.853579	31.391564	71.605953
719.004102	34.202649	71.610958
718.668969	26.320612	71.615962
717.911505	30.597792	71.620967
717.873392	24.336869	71.625972
716.894218	25.966975	71.630977
716.193562	27.595314	71.635982
715.511238	32.346229	71.640986
715.045864	33.370986	71.645991
714.301190	20.154718	71.650996
713.371635	30.049549	71.656001
712.873518	36.830620	71.661006
712.542652	33.626685	71.666010
711.438266	39.066118	71.671015
711.190814	31.192197	71.676020
710.210083	35.872357	71.681025
709.237773	27.803193	71.686030
708.694062	30.169784	71.691034
707.979680	31.653655	71.696039
707.706385	20.935902	71.701044
706.795312	41.199328	71.706049
705.989432	31.824765	71.711054
705.703623	26.481636	71.716058
705.416446	33.098235	71.721063
704.458436	30.596548	71.726068
703.277742	33.138678	71.731073
702.482866	29.363658	71.736078
702.430138	35.368922	71.741082
701.831645	39.232870	71.746087
700.763452	24.560561	71.751092
700.027150	35.843873	71.756097
699.804283	36.468901	71.761102
699.462087	22.679201	71.766106
698.136928	31.664055	71.771111
697.698022	21.092521	71.776116
697.129128	28.326403	71.781121
696.201034	25.064603	71.786126
695.575694	22.699184	71.791130
694.276213	33.605395	71.796135
694.196334	20.213898	71.801140
693.754436	25.314460	71.806145
693.209688	30.581210	71.811150
692.393196	21.347120	71.816154
691.869969	23.666297	71.821159
691.641130	30.887036	71.826164
690.299867	35.971535	71.831169
689.408784	23.649058	71.836174
689.302488	34.228089	71.841178
688.332881	27.232401	71.846183
687.578185	18.305440	71.851188
686.799177	30.161671	71.856193
686.525405	32.586209	71.861198
686.304570	28.927946	71.866202
684.912918	30.138046	71.871207
684.519611	25.901703	71.876212
684.045003	38.606750	71.881217
683.251891	27.388300	71.886222
682.448499	23.105294	71.891226
681.543771	30.301192	71.896231
681.435705	18.863283	71.901236
680.722028	30.614497	71.906241
679.899308	30.931345	71.911246
679.162581	29.439944	71.916250
678.132036	30.881127	71.921255
677.244468	29.415323	71.926260
676.541229	26.619193	71.931265
675.952113	32.506440	71.936270
675.906169	30.717389	71.941274
675.596957	32.518372	71.946279
675.163088	32.956228	71.951284
674.023086	31.052808	71.956289
673.537950	23.940561	71.961294
673.020262	20.446265	71.966298
671.606358	27.165007	71.971303
671.266341	18.832758	71.976308
670.557094	28.892789	71.981313
669.754874	29.122798	71.986318
669.179537	21.589682	71.991322
668.118761	26.952797	71.996327
668.140094	26.993321	72.001332
667.386324	26.715727	72.006337
666.676803	24.868340	72.011342
665.880447	17.485538	72.016346
665.023531	27.753585	72.021351
664.956687	24.285269	72.026356
664.114221	29.960550	72.031361
663.393008	23.620752	72.036366
662.835267	27.758910	72.041370
661.848805	39.178260	72.046375
661.393600	25.072253	72.051380
660.332592	32.113273	72.056385
659.702678	28.282038	72.061390
659.793112	17.495340	72.066394
658.538614	24.988211	72.071399
657.873657	19.918355	72.076404
657.195608	37.159532	72.081409
656.689744	30.667171	72.086414
655.888869	30.218887	72.091418
655.170632	39.198579	72.096423
654.793550	25.332444	72.101428
654.152081	31.636459	72.106433
653.529074	32.203785	72.111438
652.755670	23.510047	72.116442
652.188421	39.648651	72.121447
651.801541	27.055089	72.126452
650.780274	39.454533	72.131457
650.063411	30.337053	72.136462
649.415329	25.698168	72.141466
648.495987	45.488267	72.146471
647.807433	26.843143	72.151476
647.146339	33.289055	72.156481
646.671715	33.862716	72.161486
646.249557	32.751735	72.166490
645.641364	43.040113	72.171495
644.976497	18.168626	72.176500
644.201632	33.993359	72.181505
643.745119	34.311826	72.186510
643.176211	24.615709	72.191514
642.006671	33.291957	72.196519
641.353238	26.939795	72.201524
640.912562	32.916949	72.206529
640.076877	29.777649	72.211534
639.331312	29.654873	72.216538
638.876098	32.969317	72.221543
638.642898	25.935228	72.226548
637.122864	29.748823	72.231553
636.588638	28.058032	72.236558
636.429958	25.441697	72.241562
635.988184	31.871607	72.246567
635.162692	30.624589	72.251572
634.120194	42.038679	72.256577
633.593450	31.500068	72.261582
633.447466	28.176819	72.266586
632.174078	33.786696	72.271591
631.663183	26.413635	72.276596
631.060358	32.370881	72.281601
629.979231	29.502482	72.286606
629.407083	24.802626	72.291610
628.482565	34.113212	72.296615
628.089715	31.903172	72.301620
627.827120	33.624197	72.306625
627.100564	39.377226	72.311630
626.010960	27.173125	72.316634
625.456426	37.795152	72.321639
625.352666	42.132256	72.326644
624.358940	32.860181	72.331649
623.526573	29.788167	72.336654
623.088581	31.784704	72.341658
622.371104	33.699596	72.346663
622.228374	30.404214	72.351668
621.011873	38.887681	72.356673
620.753913	36.075847	72.361678
619.902046	29.242787	72.366682
618.701171	36.307674	72.371687
617.959625	31.508642	72.376692
618.043685	36.512840	72.381697
617.328515	38.676522	72.386702
616.235135	24.903975	72.391706
615.331212	37.718397	72.396711
615.359009	27.952488	72.401716
614.754664	41.261669	72.406721
613.807493	30.715905	72.411726
613.096467	31.573223	72.416730
612.333418	33.471721	72.421735
611.924862	41.547402	72.426740
610.700135	39.173384	72.431745
610.305302	43.750808	72.436750
610.008222	36.036193	72.441754
609.354128	33.389950	72.446759
608.297723	35.305208	72.451764
607.605413	31.308884	72.456769
606.926647	36.428262	72.461774
606.795582	31.533585	72.466778
605.780870	38.215596	72.471783
604.968304	32.478562	72.476788
604.368865	33.483689	72.481793
604.055202	33.631180	72.486798
603.758157	34.528224	72.491802
602.571098	38.161078	72.496807
602.160310	37.316374	72.501812
601.113442	29.804756	72.506817
600.444270	40.191158	72.511822
599.959669	28.966187	72.516826
599.230075	35.844062	72.521831
598.615002	29.711305	72.526836
597.388642	31.227861	72.531841
596.969439	39.453470	72.536846
596.666834	31.514238	72.541850
596.082947	37.406976	72.546855
595.241624	34.588708	72.551860
594.443235	37.096807	72.556865
593.849739	34.106606	72.561870
593.825642	25.183166	72.566874
592.379770	38.377218	72.571879
591.715907	30.907105	72.576884
590.846255	34.016329	72.581889
590.726038	33.696200	72.586894
590.503769	25.042441	72.591898
589.401528	32.432248	72.596903
588.630835	27.596869	72.601908
588.068529	32.940549	72.606913
587.259266	35.939233	72.611918
586.497324	28.973595	72.616922
585.756152	27.577547	72.621927
585.346262	32.857529	72.626932
584.963596	36.392237	72.631937
583.467939	41.214376	72.636942
583.125986	28.747718	72.641946
582.868147	36.972858	72.646951
582.590206	27.511111	72.651956
581.432965	34.389292	72.656961
580.661488	34.513510	72.661966
580.267129	28.627878	72.666970
579.529835	33.753428	72.671975
578.916781	29.634105	72.676980
578.293552	31.060916	72.681985
577.494317	27.595715	72.686990
576.800666	30.807797	72.691994
575.573529	38.739471	72.696999
575.413025	29.120250	72.702004
574.988982	31.202881	72.707009
574.195271	21.865866	72.712014
573.305645	30.719903	72.717018
572.586656	29.153171	72.722023
572.151229	23.808666	72.727028
571.746218	30.396728	72.732033
570.882410	27.313972	72.737038
570.314822	23.491761	72.742042
569.517514	36.927870	72.747047
569.132517	30.484089	72.752052
567.617055	35.954358	72.757057
566.699928	33.466716	72.762062
566.881359	25.429897	72.767066
566.148170	33.085780	72.772071
565.783059	19.979432	72.777076
564.949048	33.522308	72.782081
563.965931	27.366184	72.787086
564.058833	25.091403	72.792090
563.071109	28.394481	72.797095
561.913432	25.076264	72.802100
561.351787	34.523033	72.807105
560.923839	31.479665	72.812110
560.898760	38.866648	72.817114
559.444170	37.409201	72.822119
559.086854	23.628257	72.827124
558.671365	28.871285	72.832129
557.589490	26.777315	72.837134
556.982122	30.240584	72.842138
556.047525	35.818609	72.847143
556.151559	22.840960	72.852148
554.966975	31.994294	72.857153
553.847129	34.406952	72.862158
553.832348	26.191654	72.867162
553.148114	28.894467	72.872167
552.265099	29.175230	72.877172
551.481282	26.032432	72.882177
550.638992	28.801422	72.887182
550.655482	31.214430	72.892186
549.575259	30.416442	72.897191
548.526068	24.575199	72.902196
547.900723	34.356965	72.907201
547.746380	24.093380	72.912206
547.539403	29.402544	72.917210
546.511513	36.974489	72.922215
545.967872	27.878345	72.927220
545.432460	37.167976	72.932225
544.307752	23.618080	72.937230
543.585505	33.391627	72.942234
542.955831	28.786112	72.947239
542.674856	24.049363	72.952244
541.924545	31.928749	72.957249
540.978537	31.505197	72.962254
540.496869	29.738248	72.967258
539.967753	31.990584	72.972263
539.154341	20.731283	72.977268
538.036005	35.861699	72.982273
537.461001	33.612882	72.987278
537.325745	22.832178	72.992282
536.755392	27.114292	72.997287
536.168699	22.839399	73.002292
535.610960	31.463963	73.007297
534.606624	23.229678	73.012302
533.546019	26.221104	73.017306
532.880474	26.676965	73.022311
532.816185	29.309417	73.027316
532.247071	23.106285	73.032321
530.890606	23.989168	73.037326
530.560675	24.363185	73.042330
530.092262	35.886125	73.047335
529.216756	23.783594	73.052340
528.073683	29.628221	73.057345
527.732798	25.631138	73.062350
527.575742	31.853282	73.067354
526.742102	34.081591	73.072359
525.456022	33.291174	73.077364
525.071463	32.546383	73.082369
524.595556	34.474859	73.087374
524.441251	24.195503	73.092378
523.188624	33.214610	73.097383
522.381051	33.005554	73.102388
522.178252	38.211556	73.107393
521.514642	30.884928	73.112398
520.763514	30.307340	73.117402
519.663350	36.641872	73.122407
519.398229	35.102203	73.127412
518.958864	28.583518	73.132417
517.833667	33.384525	73.137422
517.673963	28.830308	73.142426
516.765773	37.993247	73.147431
515.881846	31.378223	73.152436
514.965002	37.631516	73.157441
514.404718	34.203966	73.162446
514.172683	39.305816	73.167450
513.653167	32.104469	73.172455
512.488948	25.769063	73.177460
511.926160	31.086024	73.182465
510.981039	34.571568	73.187470
510.875552	25.612217	73.192474
510.345325	29.722365	73.197479
509.413756	28.731983	73.202484
508.779516	31.288073	73.207489
508.270136	27.265796	73.212494
506.786327	25.291070	73.217498
506.182395	27.593177	73.222503
506.147046	27.109724	73.227508
505.578268	24.270151	73.232513
504.764803	28.212534	73.237518
504.391007	23.586771	73.242522
503.325587	35.466588	73.247527
502.716290	24.947483	73.252532
502.136280	29.276873	73.257537
501.615791	32.256387	73.262542
500.843087	23.824370	73.267546
499.858988	29.735145	73.272551
499.645894	20.980597	73.277556
499.055171	26.757742	73.282561
498.283756	27.500134	73.287566
497.953557	28.399317	73.292570
496.660391	25.189448	73.297575
496.001097	26.319252	73.302580
495.474578	22.432172	73.307585
494.823902	27.783636	73.312590
494.572245	26.889947	73.317594
493.088323	33.949513	73.322599
492.979884	28.251738	73.327604
492.559390	32.748105	73.332609
491.860669	31.961906	73.337614
490.898088	21.406049	73.342618
490.103757	34.734463	73.347623
489.686047	21.455168	73.352628
488.749825	22.796245	73.357633
487.462083	32.475388	73.362638
487.604814	24.936741	73.367642
486.990244	32.384510	73.372647
486.869624	30.347168	73.377652
485.699429	21.082784	73.382657
484.883996	38.057284	73.387662
484.648683	28.464189	73.392666
483.521851	33.708589	73.397671
482.769527	31.563728	73.402676
482.222593	32.782867	73.407681
481.397391	26.349314	73.412686
481.355586	30.723852	73.417690
480.387969	34.080527	73.422695
479.609254	22.607569	73.427700
479.085985	27.462504	73.432705
478.512523	33.124943	73.437710
477.490587	23.833788	73.442714
476.577097	32.798885	73.447719
476.480986	33.113581	73.452724
476.112188	29.668151	73.457729
475.231508	22.240509	73.462734
474.521786	19.757710	73.467738
473.663074	27.165528	73.472743
473.067785	21.529550	73.477748
472.063873	26.929409	73.482753
471.157591	29.962506	73.487758
471.310856	20.007895	73.492762
470.535298	33.434245	73.497767
470.018114	21.720931	73.502772
469.042013	24.487610	73.507777
468.499161	33.172889	73.512782
468.196696	24.229158	73.517786
466.857170	28.793097	73.522791
466.194386	20.629010	73.527796
465.827977	23.473595	73.532801
465.005898	29.730725	73.537806
464.641013	21.637448	73.542810
463.590418	28.795145	73.547815
463.039367	24.035206	73.552820
462.735000	26.627059	73.557825
461.828975	28.132067	73.562830
461.073969	27.768002	73.567834
460.278578	26.930982	73.572839
460.417211	23.094056	73.577844
459.435815	17.954833	73.582849
458.290092	26.239425	73.587854
457.737051	24.528019	73.592858
456.927549	26.602694	73.597863
456.955069	25.849031	73.602868
456.006535	23.989328	73.607873
454.977238	27.343222	73.612878
454.822812	27.238283	73.617882
454.131758	32.400650	73.622887
453.204928	14.951068	73.627892
452.457616	23.968537	73.632897
451.990595	23.919710	73.637902
451.300359	30.329301	73.642906
450.551978	27.415856	73.647911
450.232467	19.696972	73.652916
449.521218	23.427544	73.657921
448.650955	27.612379	73.662926
447.967922	26.834732	73.667930
447.269245	32.499780	73.672935
446.835938	23.326167	73.677940
445.751281	26.807156	73.682945
444.796728	29.253447	73.687950
444.834089	23.450449	73.692954
444.397911	28.504400	73.697959
443.293098	24.326275	73.702964
442.471363	35.202201	73.707969
441.998428	31.834868	73.712974
441.773857	27.046571	73.717978
440.406266	32.602157	73.722983
439.960088	29.399294	73.727988
439.579690	30.117250	73.732993
438.761437	28.350335	73.737998
437.879909	25.046528	73.743002
437.041173	34.600539	73.748007
436.790797	25.763630	73.753012
436.417721	30.198832	73.758017
435.518917	23.497908	73.763022
434.968676	18.919197	73.768026
434.192262	25.323597	73.773031
433.332148	22.912080	73.778036
432.726057	27.750257	73.783041
431.792570	29.245459	73.788046
431.566798	20.138133	73.793050
431.122161	25.742205	73.798055
430.433829	25.728643	73.803060
429.469203	26.339416	73.808065
428.777635	28.776927	73.813070
428.001475	23.753247	73.818074
426.947750	24.986914	73.823079
426.546683	21.317980	73.828084
425.821217	22.117727	73.833089
425.643286	28.084577	73.838094
425.385007	23.856735	73.843098
424.318845	27.935597	73.848103
423.562369	23.952713	73.853108
422.996473	23.440257	73.858113
422.179997	24.066851	73.863118
421.900725	26.996904	73.868122
420.730865	30.414209	73.873127
420.390835	29.233415	73.878132
419.106471	29.846252	73.883137
418.634965	30.603959	73.888142
418.453113	24.031654	73.893146
417.764073	30.120944	73.898151
416.741320	25.235906	73.903156
415.813940	28.742309	73.908161
415.278049	28.436383	73.913166
415.145992	27.796455	73.918170
414.601204	36.042087	73.923175
413.875570	31.029282	73.928180
413.031931	23.579996	73.933185
412.416549	20.438795	73.938190
411.648962	18.597586	73.943194
410.793090	21.073895	73.948199
410.408474	17.211536	73.953204
410.290153	22.889769	73.958209
409.339346	20.041710	73.963214
408.460915	20.966758	73.968218
407.747400	37.093984	73.973223
406.650930	31.828038	73.978228
406.081967	32.371043	73.983233
405.152508	30.509897	73.988238
404.994622	17.239693	73.993242
404.940125	29.781611	73.998247
403.607561	30.911487	74.003252
402.721392	23.893177	74.008257
402.281340	30.091028	74.013262
402.258104	26.089084	74.018266
401.420039	32.495434	74.023271
400.611712	23.439938	74.028276
399.880084	31.321108	74.033281
399.020696	38.005246	74.038286
398.149342	24.612184	74.043290
397.643872	37.492470	74.048295
397.751890	29.399542	74.053300
396.458637	33.946682	74.058305
395.263756	26.299484	74.063310
394.760590	19.679038	74.068314
394.043467	26.589658	74.073319
393.973216	24.790298	74.078324
393.363924	27.348747	74.083329
392.562800	34.572373	74.088334
392.092028	31.893828	74.093338
391.295698	24.468551	74.098343
390.761233	18.450751	74.103348
389.601433	20.595457	74.108353
389.380045	24.678488	74.113358
388.635358	22.854137	74.118362
387.575140	24.531973	74.123367
386.962654	30.739957	74.128372
386.591285	20.469986	74.133377
386.020582	26.243961	74.138382
385.123724	23.270620	74.143386
384.038818	29.113920	74.148391
383.793709	32.172573	74.153396
383.589306	32.722145	74.158401
382.669625	31.072335	74.163406
382.013067	26.434885	74.168410
381.263764	34.131221	74.173415
380.718693	22.058109	74.178420
379.859895	28.032534	74.183425
379.020755	30.115109	74.188430
378.823408	17.519818	74.193434
378.240211	29.947290	74.198439
377.415073	25.620553	74.203444
376.776584	29.390012	74.208449
376.020759	29.757800	74.213454
375.568484	28.721053	74.218458
374.488892	30.327867	74.223463
374.040948	22.738272	74.228468
373.496059	26.456546	74.233473
372.144954	32.733350	74.238478
371.645400	20.772837	74.243482
371.011443	30.041917	74.248487
370.774200	26.148194	74.253492
370.189572	22.308253	74.258497
369.416118	32.186184	74.263502
369.026533	24.940523	74.268506
368.323331	20.824592	74.273511
367.487953	23.478997	74.278516
366.436268	28.501734	74.283521
365.949777	31.291352	74.288526
365.962974	23.861659	74.293530
364.739301	26.975330	74.298535
363.665968	25.392591	74.303540
363.421825	25.811305	74.308545
362.800925	35.073578	74.313550
362.570214	21.304058	74.318554
361.402846	29.122211	74.323559
360.864188	22.244081	74.328564
360.367775	25.308090	74.333569
359.229128	26.610510	74.338574
358.519493	18.763008	74.343578
357.994857	27.629896	74.348583
357.739694	27.506324	74.353588
357.182829	24.821007	74.358593
355.923681	20.186558	74.363598
355.583519	19.453643	74.368602
354.985021	30.568395	74.373607
354.118226	29.190862	74.378612
353.364196	23.334216	74.383617
352.702524	30.359011	74.388622
352.559866	16.297925	74.393626
351.290833	27.938998	74.398631
350.658357	17.855727	74.403636
350.171062	18.251690	74.408641
349.585861	27.740081	74.413646
349.115584	20.843173	74.418650
348.213995	26.644655	74.423655
347.587158	22.827216	74.428660
347.340314	27.381079	74.433665
345.924109	27.947157	74.438670
345.508343	19.808401	74.443674
344.759089	27.738120	74.448679
344.245723	27.002848	74.453684
344.295223	24.949444	74.458689
342.552515	22.429461	74.463694
342.225303	15.683220	74.468698
341.361793	29.169335	74.473703
341.165116	26.735699	74.478708
340.116941	25.521117	74.483713
339.186968	28.826111	74.488718
338.999594	22.160082	74.493722
338.404797	31.474967	74.498727
338.044960	28.583215	74.503732
337.236925	23.362801	74.508737
336.443111	27.409331	74.513742
335.798087	24.123066	74.518746
334.369484	30.104737	74.523751
333.917762	22.283946	74.528756
333.331349	33.715317	74.533761
333.432086	35.346924	74.538766
332.990515	23.238410	74.543770
331.765693	26.084201	74.548775
330.942472	26.680360	74.553780
330.838855	32.362560	74.558785
329.875028	35.308682	74.563790
329.043815	24.621584	74.568794
328.236369	27.217934	74.573799
327.619291	27.237199	74.578804
326.756917	29.287224	74.583809
325.977771	28.452391	74.588814
325.790538	10.511282	74.593818
325.257258	25.274118	74.598823
325.003276	28.383074	74.603828
324.135594	23.714636	74.608833
323.244656	34.577961	74.613838
322.262622	29.464128	74.618842
321.224505	41.571462	74.623847
320.747344	28.006802	74.628852
320.144639	26.014767	74.633857
319.782108	34.671327	74.638862
319.707067	24.172795	74.643866
318.818528	28.981894	74.648871
318.050141	19.308221	74.653876
317.501118	27.168186	74.658881
316.458374	34.021915	74.663886
315.816269	28.923293	74.668890
315.205392	29.490346	74.673895
314.722605	26.947773	74.678900
314.022997	22.747709	74.683905
312.717876	28.017436	74.688910
312.680080	22.693195	74.693914
311.897743	34.209410	74.698919
311.276784	24.207891	74.703924
310.395127	23.600710	74.708929
309.551250	26.127179	74.713934
309.088896	22.222036	74.718938
308.894085	30.585361	74.723943
308.187188	26.388037	74.728948
307.302036	26.178801	74.733953
306.744680	35.643841	74.738958
306.185608	28.002588	74.743962
304.846337	37.084480	74.748967
304.320671	28.116434	74.753972
303.931604	24.070302	74.758977
303.402039	23.477968	74.763982
303.018584	20.788682	74.768986
301.823354	30.953043	74.773991
301.565779	27.253379	74.778996
301.123200	22.995006	74.784001
299.981661	31.905035	74.789006
299.522398	24.599535	74.794010
298.630224	37.580885	74.799015
297.801441	24.740899	74.804020
297.047855	28.549220	74.809025
296.550942	30.263466	74.814030
296.287470	25.659583	74.819034
295.523463	26.791934	74.824039
294.576813	21.344476	74.829044
293.949115	24.139265	74.834049
293.395126	27.354385	74.839054
293.124214	24.178813	74.844058
291.960300	28.908811	74.849063
291.227351	22.438555	74.854068
290.900370	27.850429	74.859073
290.179182	25.741670	74.864078
289.390711	19.650845	74.869082
288.409258	32.510807	74.874087
288.184703	14.542537	74.879092
287.813805	18.759787	74.884097
286.584727	27.447231	74.889102
286.135213	26.381677	74.894106
285.316277	27.070208	74.899111
285.004967	30.931038	74.904116
284.270427	36.783187	74.909121
283.161023	23.087510	74.914126
282.853753	26.995004	74.919130
282.125021	37.613293	74.924135
281.587258	26.171399	74.929140
281.100828	24.405264	74.934145
280.132204	35.162713	74.939150
280.082991	29.908100	74.944154
278.644026	30.318574	74.949159
278.118291	29.001823	74.954164
277.840492	35.076057	74.959169
276.918277	34.672469	74.964174
276.314652	29.447879	74.969178
275.345604	34.741328	74.974183
274.581393	37.595730	74.979188
274.695404	30.131048	74.984193
273.465271	33.209523	74.989198
272.723516	24.225470	74.994202
271.932863	26.522698	74.999207
271.949779	26.996001	75.004212
271.330200	32.429286	75.009217
270.042202	34.553481	75.014222
270.019795	34.258778	75.019226
269.167084	40.702194	75.024231
268.409005	26.930022	75.029236
267.617797	28.875684	75.034241
267.092132	33.675843	75.039246
266.503771	27.559434	75.044250
265.385259	37.741547	75.049255
264.550784	31.377366	75.054260
264.148730	36.101053	75.059265
263.873634	28.271048	75.064270
263.209615	25.970260	75.069274
262.426530	32.896156	75.074279
261.712336	29.045358	75.079284
261.448506	23.856497	75.084289
260.127602	19.334445	75.089294
259.405706	13.624102	75.094298
258.846951	23.045208	75.099303
258.787150	27.687531	75.104308
257.844887	30.765857	75.109313
256.945552	24.227520	75.114318
256.344652	17.474460	75.119322
255.901386	24.335147	75.124327
254.811880	25.183510	75.129332
254.543894	30.007249	75.134337
253.658373	27.202462	75.139342
253.533795	14.239216	75.144346
252.106301	27.258591	75.149351
251.440856	25.976732	75.154356
251.212432	27.514148	75.159361
250.793471	24.666530	75.164366
250.414403	21.716360	75.169370
248.985725	24.265106	75.174375
248.609131	23.730400	75.179380
248.167253	26.065077	75.184385
247.031383	28.299071	75.189390
246.550122	26.281388	75.194394
245.925504	27.213342	75.199399
245.374785	22.079678	75.204404
244.514239	24.623017	75.209409
243.380274	26.481399	75.214414
243.204299	23.683357	75.219418
242.536376	28.685966	75.224423
241.818423	22.072992	75.229428
241.088736	20.929108	75.234433
240.664256	31.418477	75.239438
240.278181	25.583640	75.244442
239.241606	31.386175	75.249447
238.620397	27.205175	75.254452
238.331875	20.097977	75.259457
236.999621	35.582695	75.264462
236.453030	24.249456	75.269466
235.406827	33.604776	75.274471
235.134993	19.692036	75.279476
234.959127	24.133666	75.284481
234.229216	27.080378	75.289486
233.539402	16.068018	75.294490
232.912625	24.058658	75.299495
232.094668	33.606249	75.304500
231.100845	25.211168	75.309505
230.208767	37.501821	75.314510
230.178746	20.434517	75.319514
229.526731	22.362730	75.324519
228.319721	19.353741	75.329524
227.560302	28.898306	75.334529
227.320551	25.497005	75.339534
227.198233	28.848326	75.344538
226.264989	33.372848	75.349543
225.400813	34.215265	75.354548
224.657220	34.579572	75.359553
224.265923	33.034823	75.364558
223.717062	31.378000	75.369562
222.737761	33.084005	75.374567
222.046037	28.750250	75.379572
221.180649	24.084642	75.384577
220.121301	22.758356	75.389582
219.951134	17.362187	75.394586
219.061336	25.079374	75.399591
218.734591	21.780252	75.404596
218.527277	20.964679	75.409601
217.546488	21.289531	75.414606
217.158024	20.408221	75.419610
216.312525	18.894883	75.424615
215.470238	14.985678	75.429620
214.705128	19.721513	75.434625
213.791698	26.363849	75.439630
213.730797	13.004113	75.444634
212.801945	20.866296	75.449639
211.946555	24.533174	75.454644
211.637545	19.010909	75.459649
210.799602	17.180982	75.464654
210.668881	12.358838	75.469658
209.647605	23.643501	75.474663
208.985466	17.672915	75.479668
208.377199	23.642139	75.484673
207.008057	26.529919	75.489678
206.531101	16.976988	75.494682
205.822942	24.132219	75.499687
205.401594	20.193755	75.504692
205.399417	20.037752	75.509697
204.368905	12.140543	75.514702
203.703852	6.932084	75.519706
203.107995	17.522882	75.524711
202.103510	20.686838	75.529716
201.202071	19.139846	75.534721
200.732625	16.705559	75.539726
200.374852	16.172591	75.544730
200.120372	22.853378	75.549735
199.331140	22.417580	75.554740
198.603358	22.434027	75.559745
197.537619	24.907593	75.564750
196.884813	17.197747	75.569754
196.245425	26.089255	75.574759
195.935495	29.402678	75.579764
195.528138	25.239637	75.584769
194.158035	18.705421	75.589774
193.598705	19.559170	75.594778
193.168221	25.829632	75.599783
192.342605	19.038302	75.604788
191.657895	15.395716	75.609793
190.835560	20.880260	75.614798
190.699438	14.425280	75.619802
189.578509	29.226623	75.624807
188.658675	17.522410	75.629812
188.393328	21.008494	75.634817
187.716029	23.399635	75.639822
187.347727	15.486742	75.644826
186.422495	29.217690	75.649831
185.540324	28.178557	75.654836
185.249950	26.513648	75.659841
184.409083	30.597685	75.664846
183.728592	24.317798	75.669850
182.990438	25.408215	75.674855
182.597588	19.016241	75.679860
182.141534	19.774681	75.684865
181.132273	31.645637	75.689870
180.717105	19.692235	75.694874
179.961736	24.738759	75.699879
178.686594	28.411071	75.704884
178.077662	20.826696	75.709889
177.476580	23.506883	75.714894
177.259654	18.889292	75.719898
176.969153	21.138344	75.724903
176.139867	23.753991	75.729908
175.370849	21.212931	75.734913
174.323650	32.798207	75.739918
174.038247	18.717339	75.744922
172.673064	27.216798	75.749927
172.137761	26.262713	75.754932
171.858129	16.982680	75.759937
171.125044	31.414693	75.764942
171.001420	18.359845	75.769946
169.675699	22.495957	75.774951
169.109103	22.207596	75.779956
168.996339	17.316361	75.784961
167.378047	24.200400	75.789966
167.214522	21.151226	75.794970
166.571263	22.584480	75.799975
166.253627	24.140857	75.804980
165.406953	22.436916	75.809985
164.424725	26.764266	75.814990
164.296549	16.925507	75.819994
163.610593	24.004668	75.824999
162.290232	23.822297	75.830004
162.308933	16.645631	75.835009
161.190755	27.638260	75.840014
161.177385	16.138036	75.845018
159.952741	21.098539	75.850023
159.261973	28.118547	75.855028
158.664232	16.019225	75.860033
157.586443	21.237007	75.865038
156.850577	15.388580	75.870042
156.429094	27.888057	75.875047
155.907490	18.581952	75.880052
155.604363	21.572599	75.885057
155.074909	19.242505	75.890062
154.246801	14.126289	75.895066
153.500410	18.100652	75.900071
152.843249	27.163732	75.905076
151.856957	15.640444	75.910081
151.198579	25.329758	75.915086
150.945309	20.471965	75.920090
150.239737	20.461230	75.925095
149.566701	17.915915	75.930100
148.615541	20.875849	75.935105
147.809141	18.615145	75.940110
147.741537	19.153961	75.945114
146.620706	19.584748	75.950119
145.792768	19.213486	75.955124
145.634103	16.223463	75.960129
144.961587	20.309050	75.965134
144.458911	19.305617	75.970138
143.647737	28.006909	75.975143
142.673270	22.049874	75.980148
142.478591	23.186108	75.985153
141.055003	22.234897	75.990158
140.343221	18.178757	75.995162
140.105920	30.991063	76.000167
139.614497	22.807653	76.005172
139.274718	21.098590	76.010177
138.013670	31.076391	76.015182
137.405305	22.916359	76.020186
137.097598	18.146095	76.025191
136.310795	14.595498	76.030196
135.709600	12.809850	76.035201
134.773391	20.334188	76.040206
134.487828	16.471859	76.045210
133.363582	17.324236	76.050215
132.713107	18.865880	76.055220
132.431256	11.845951	76.060225
131.794440	22.227253	76.065230
131.116846	24.269955	76.070234
129.975199	25.695957	76.075239
129.619783	20.649454	76.080244
129.071353	17.701082	76.085249
128.021996	25.722853	76.090254
127.210358	15.594118	76.095258
126.987397	17.786674	76.100263
126.413515	18.970759	76.105268
126.008886	12.227448	76.110273
124.724112	20.206332	76.115278
124.626931	20.056017	76.120282
123.879391	19.872212	76.125287
122.902851	22.197546	76.130292
122.141838	17.835453	76.135297
121.568463	23.204627	76.140302
121.469294	10.078089	76.145306
120.174048	17.997144	76.150311
119.318945	23.357626	76.155316
119.091460	11.511514	76.160321
118.595615	17.529056	76.165326
118.207664	15.077060	76.170330
117.004654	19.841747	76.175335
116.165837	20.241771	76.180340
116.048248	16.578160	76.185345
114.710246	29.080287	76.190350
114.191944	23.632411	76.195354
113.685924	29.101233	76.200359
113.234253	23.576502	76.205364
112.866149	20.600956	76.210369
111.660660	30.424830	76.215374
111.403988	19.766064	76.220378
110.412693	29.825438	76.225383
109.515268	19.448618	76.230388
109.292390	24.019170	76.235393
108.349658	30.637828	76.240398
107.884643	23.215027	76.245402
107.038639	30.901610	76.250407
106.298594	23.200973	76.255412
105.809545	21.452641	76.260417
105.019392	34.331031	76.265422
104.982634	20.147454	76.270426
103.461835	21.950891	76.275431
102.669872	26.520730	76.280436
102.808925	20.259994	76.285441
102.133770	24.979938	76.290446
101.395101	20.156980	76.295450
100.460973	31.043013	76.300455
100.230235	27.865792	76.305460
99.461188	23.575949	76.310465
98.258692	26.588597	76.315470
97.942694	17.297032	76.320474
97.268267	24.642446	76.325479
95.981388	23.929654	76.330484
95.710233	20.503418	76.335489
95.054485	27.853740	76.340494
94.629101	25.644256	76.345498
94.334787	26.561420	76.350503
93.475158	21.812946	76.355508
93.260390	25.205817	76.360513
92.177654	33.800622	76.365518
91.198166	17.577031	76.370522
90.556328	26.024253	76.375527
90.093721	32.268312	76.380532
89.459910	19.950841	76.385537
88.126917	26.497699	76.390542
87.758245	22.028897	76.395546
87.220004	27.274205	76.400551
86.668397	23.255615	76.405556
86.776377	14.853638	76.410561
85.229499	30.658057	76.415566
85.021487	23.834510	76.420570
84.021618	29.962401	76.425575
82.825424	32.247088	76.430580
82.411232	21.749063	76.435585
81.855821	28.444731	76.440590
81.366503	32.160504	76.445594
81.024808	28.661941	76.450599
80.052013	27.019144	76.455604
79.234966	23.074425	76.460609
78.735322	38.760734	76.465614
78.249994	25.380387	76.470618
77.245060	31.881244	76.475623
76.595829	25.804563	76.480628
76.142649	16.608996	76.485633
75.618997	18.267622	76.490638
74.781255	28.502787	76.495642
73.664125	27.949014	76.500647
73.315928	25.722494	76.505652
73.079625	24.898942	76.510657
72.204539	35.171606	76.515662
71.421911	25.880343	76.520666
70.856959	29.884141	76.525671
70.350303	35.335726	76.530676
69.691009	26.111526	76.535681
68.880289	27.434319	76.540686
68.726867	27.707706	76.545690
67.474495	36.618152	76.550695
66.303518	30.435449	76.555700
66.172050	25.733282	76.560705
65.432685	28.418200	76.565710
65.068697	37.852433	76.570714
64.225125	34.886489	76.575719
63.569721	24.734437	76.580724
63.122766	25.850987	76.585729
62.227891	30.544482	76.590734
61.442630	25.331581	76.595738
60.756204	31.463107	76.600743
60.020572	26.076714	76.605748
60.176679	19.731258	76.610753
59.258770	33.533610	76.615758
58.588290	31.505144	76.620762
57.662637	38.611522	76.625767
56.316482	28.695787	76.630772
55.630808	22.659619	76.635777
55.141574	37.461189	76.640782
55.061354	31.363150	76.645786
54.556818	37.382094	76.650791
53.997293	29.583299	76.655796
53.073255	26.914041	76.660801
51.999700	34.389354	76.665806
52.061799	22.918104	76.670810
51.309925	27.459487	76.675815
50.113541	40.315949	76.680820
50.148191	29.856729	76.685825
49.332404	32.889726	76.690830
48.225430	25.879979	76.695834
47.453706	31.022186	76.700839
46.839010	30.631140	76.705844
46.709956	37.055394	76.710849
45.525391	39.443899	76.715854
45.015974	25.863981	76.720858
44.369307	24.751072	76.725863
43.843989	26.663856	76.730868
43.264556	24.507336	76.735873
42.123005	26.933134	76.740878
41.422381	30.136997	76.745882
41.785630	35.719501	76.750887
40.704837	30.940088	76.755892
39.952701	23.682944	76.760897
38.994411	25.109705	76.765902
37.753567	20.666477	76.770906
37.476223	28.027420	76.775911
36.834472	30.586392	76.780916
36.628801	15.414230	76.785921
35.911043	29.869047	76.790926
35.462873	20.672690	76.795930
34.454080	28.591832	76.800935
33.720045	25.926971	76.805940
33.642961	24.934529	76.810945
32.495908	22.297696	76.815950
31.789987	17.622502	76.820954
31.009463	25.178812	76.825959
30.580847	28.178448	76.830964
30.009473	20.047246	76.835969
29.241942	23.913053	76.840974
28.732071	23.412255	76.845978
28.148645	26.176388	76.850983
26.876554	33.580875	76.855988
26.600360	26.940096	76.860993
26.016683	33.786937	76.865998
25.630525	29.030779	76.871002
24.462999	23.098283	76.876007
23.885391	28.140150	76.881012
23.570371	20.100525	76.886017
22.350191	27.592924	76.891022
21.663886	21.552138	76.896026
20.862814	23.452138	76.901031
20.517201	31.044741	76.906036
20.705049	25.708185	76.911041
19.327665	25.574410	76.916046
18.779042	22.381672	76.921050
18.042956	26.644584	76.926055
17.401500	25.210734	76.931060
16.544244	28.688740	76.936065
15.918303	32.032084	76.941070
15.570609	26.815638	76.946074
14.497496	34.079586	76.951079
13.456107	28.939092	76.956084
13.127064	26.203333	76.961089
12.613784	35.877418	76.966094
12.527714	22.704646	76.971098
11.323791	22.927978	76.976103
10.335120	30.137456	76.981108
10.065210	25.091529	76.986113
9.371090	29.759328	76.991118
9.158651	27.369242	76.996122
8.432293	24.348356	77.001127
7.704622	27.009347	77.006132
6.830683	23.901617	77.011137
5.962580	26.711163	77.016142
5.659529	20.267059	77.021147
4.929659	32.429387	77.026151
3.956431	21.230513	77.031156
3.194080	16.247368	77.036161