Mon Mar 08 17:53:45 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.390101	86.570345	0.000000
-1.366299	86.312808	0.005005
-2.424261	54.659242	0.010010
-3.569725	3.181993	0.015014
-8.057518	-7.564679	0.020019
-13.503082	-14.741372	0.025024
-18.504826	-10.704397	0.030029
-23.475228	-5.937564	0.035034
-27.056161	-15.745503	0.040038
-30.701419	-6.591734	0.045043
-34.441841	-10.391382	0.050048
-38.027561	-14.950546	0.055053
-41.870022	-7.597686	0.060058
-45.319677	-12.806159	0.065062
-49.169271	-4.152766	0.070067
-53.072847	-3.233439	0.075072
-56.630622	-7.587305	0.080077
-60.885105	-6.643524	0.085082
-64.543001	-8.863599	0.090086
-68.242597	-7.946828	0.095091
-71.995951	-12.644774	0.100096
-75.561461	-13.100804	0.105101
-79.356136	-7.695123	0.110106
-83.059681	2.294330	0.115110
-87.113565	-3.364880	0.120115
-90.689194	-12.432414	0.125120
-93.969789	-11.445260	0.130125
-98.405874	-12.326899	0.135130
-101.989104	-3.268078	0.140134
-105.495645	-8.317580	0.145139
-109.642789	-15.314864	0.150144
-113.251660	-13.611424	0.155149
-117.367869	-6.930695	0.160154
-120.896581	-10.920099	0.165158
-124.361855	-8.957286	0.170163
-127.955389	-7.773501	0.175168
-131.898064	-12.822758	0.180173
-136.175338	-15.393317	0.185178
-139.459305	-27.216449	0.190182
-143.305995	-21.236263	0.195187
-147.407269	-19.791664	0.200192
-151.505035	-21.012611	0.205197
-155.209564	-6.445110	0.210202
-158.806702	-14.476220	0.215206
-162.826281	-9.627448	0.220211
-166.067757	-14.838999	0.225216
-169.786673	-13.449069	0.230221
-173.456686	-6.202375	0.235226
-176.819665	-18.413387	0.240230
-180.666570	-1.850403	0.245235
-184.829679	-5.591822	0.250240
-188.607985	-17.738116	0.255245
-192.336247	-8.578760	0.260250
-196.337492	-16.445976	0.265254
-199.886235	-11.399476	0.270259
-203.596283	-9.712871	0.275264
-206.967944	-1.452474	0.280269
-211.614039	-7.218800	0.285274
-214.620130	-11.357699	0.290278
-218.633224	-7.596367	0.295283
-222.616528	-7.064582	0.300288
-226.133042	-10.500699	0.305293
-230.016179	0.578890	0.310298
-233.645329	-4.900274	0.315302
-237.541548	-5.561898	0.320307
-241.317269	-5.809094	0.325312
-244.822499	-4.719653	0.330317
-249.146968	-3.786450	0.335322
-252.384899	-7.435723	0.340326
-256.449800	0.522235	0.345331
-260.432872	-4.905128	0.350336
-263.402594	-6.011050	0.355341
-267.527742	-0.703719	0.360346
-271.182233	-7.905503	0.365350
-275.107292	-2.418791	0.370355
-278.905993	-6.673939	0.375360
-282.405851	-12.189430	0.380365
-286.893763	-3.340754	0.385370
-290.437841	-10.211632	0.390374
-294.059133	-6.643603	0.395379
-297.765132	-7.027993	0.400384
-301.372192	-3.867492	0.405389
-305.285437	1.041808	0.410394
-308.896809	-3.662656	0.415398
-312.623740	2.557295	0.420403
-316.553355	-5.229690	0.425408
-319.871916	-9.234995	0.430413
-323.763399	1.554337	0.435418
-327.853507	-1.638679	0.440422
-331.459253	-1.654254	0.445427
-335.263874	-11.604187	0.450432
-338.897639	-6.860875	0.455437
-342.868025	-4.381884	0.460442
-346.390153	-13.996859	0.465446
-350.361552	-7.184330	0.470451
-354.036239	-14.573561	0.475456
-357.767671	-10.601510	0.480461
-361.923302	-3.600280	0.485466
-365.460020	-22.190271	0.490470
-369.187468	-10.274344	0.495475
-373.086886	-3.607308	0.500480
-376.824856	-12.186432	0.505485
-380.576313	-17.325719	0.510490
-384.002432	-16.428476	0.515494
-387.897782	-9.121841	0.520499
-391.839275	-12.606546	0.525504
-395.560377	-16.509623	0.530509
-399.672674	-9.606713	0.535514
-403.076913	-14.137523	0.540518
-406.815545	-11.821587	0.545523
-410.301865	-9.333048	0.550528
-413.907391	-12.330480	0.555533
-418.059459	0.578976	0.560538
-421.926858	-4.732542	0.565542
-425.895437	-1.135671	0.570547
-429.389705	-4.201307	0.575552
-432.609211	-9.343455	0.580557
-436.805491	-10.619142	0.585562
-440.572431	-5.584763	0.590566
-444.724626	-7.111898	0.595571
-448.468553	-12.097741	0.600576
-451.858664	-10.360926	0.605581
-455.920557	1.277391	0.610586
-459.169922	-6.614824	0.615590
-463.115162	-9.701429	0.620595
-467.025691	-10.079701	0.625600
-470.624349	-8.834667	0.630605
-474.736809	-7.865532	0.635610
-478.647283	3.228258	0.640614
-482.189646	5.393122	0.645619
-485.615457	3.783166	0.650624
-489.158103	1.769262	0.655629
-493.367481	4.759743	0.660634
-496.948532	-4.864512	0.665638
-501.017757	-3.233626	0.670643
-504.824433	-2.497776	0.675648
-508.211339	-2.147500	0.680653
-512.207241	-0.881534	0.685658
-515.833139	-12.770923	0.690662
-519.832733	-1.878877	0.695667
-523.473652	-0.477207	0.700672
-527.192425	-2.153847	0.705677
-531.363725	5.011016	0.710682
-534.535514	-1.239299	0.715686
-537.973025	-7.494472	0.720691
-542.169884	0.980174	0.725696
-545.324529	-7.584617	0.730701
-549.728586	5.516687	0.735706
-553.448898	-14.708891	0.740710
-557.061525	-3.325104	0.745715
-561.264935	-1.117609	0.750720
-565.103064	2.247345	0.755725
-568.898769	3.919808	0.760730
-572.169441	-0.403440	0.765734
-576.398485	-0.213425	0.770739
-580.034903	-8.097249	0.775744
-583.383031	-8.434287	0.780749
-587.343874	-1.684565	0.785754
-590.858554	-8.785170	0.790758
-594.936494	-0.458740	0.795763
-598.535559	-13.976497	0.800768
-601.911817	-3.994437	0.805773
-606.269623	4.362531	0.810778
-609.871708	-2.873891	0.815782
-613.775636	-6.493530	0.820787
-617.920824	-4.050816	0.825792
-621.399893	-12.456435	0.830797
-624.843168	-4.002702	0.835802
-628.415444	-9.126060	0.840806
-632.731019	5.107663	0.845811
-636.612339	-1.131649	0.850816
-639.997338	-11.859291	0.855821
-643.660947	4.623036	0.860826
-647.430539	-1.615184	0.865830
-651.134006	-1.471164	0.870835
-655.219558	-5.615210	0.875840
-658.377117	-9.212103	0.880845
-663.154765	-6.300839	0.885850
-666.312934	-11.121305	0.890854
-669.798036	-9.613426	0.895859
-673.882726	-12.936005	0.900864
-677.369460	-8.641454	0.905869
-681.812093	-6.040719	0.910874
-684.993607	-11.472425	0.915878
-689.180276	-6.264945	0.920883
-692.763326	-9.456342	0.925888
-696.180389	-10.914426	0.930893
-700.537458	-8.596981	0.935898
-703.685746	-14.762500	0.940902
-707.647883	-13.865870	0.945907
-711.569905	-3.881606	0.950912
-715.323722	-12.646863	0.955917
-719.126926	2.244694	0.960922
-722.942817	-8.697807	0.965926
-726.625601	-2.350257	0.970931
-730.046568	-0.183929	0.975936
-734.086237	-2.797682	0.980941
-738.015061	-11.834546	0.985946
-741.477653	-15.802032	0.990950
-745.065258	-2.531268	0.995955
-748.985043	-3.975163	1.000960
-752.739021	-8.380178	1.005965
-756.509874	1.952150	1.010970
-760.536564	-9.278286	1.015974
-764.231067	-4.303872	1.020979
-768.134485	-13.765776	1.025984
-771.726751	-10.627444	1.030989
-775.348722	5.903601	1.035994
-779.142164	-1.062275	1.040998
-783.084592	0.405326	1.046003
-787.049177	1.419171	1.051008
-790.575709	-3.824784	1.056013
-794.600347	-1.869374	1.061018
-797.988246	-3.062320	1.066022
-801.468596	-2.081695	1.071027
-805.458019	2.011123	1.076032
-809.096958	-8.044906	1.081037
-813.156063	0.606866	1.086042
-816.827707	-12.082087	1.091046
-820.637123	-0.295900	1.096051
-824.667891	-2.265962	1.101056
-827.826168	-5.741085	1.106061
-831.696826	-8.140416	1.111066
-835.521944	0.022994	1.116070
-839.357776	0.167968	1.121075
-843.521362	-2.378477	1.126080
-846.873113	-5.075193	1.131085
-851.117273	-9.720222	1.136090
-854.351813	-8.985390	1.141094
-857.875718	-0.723446	1.146099
-861.738155	-6.862888	1.151104
-865.260474	-12.902158	1.156109
-869.643775	-6.026104	1.161114
-873.035743	-1.681769	1.166118
-877.317059	-7.303223	1.171123
-880.835736	-4.775717	1.176128
-884.586885	-11.223061	1.181133
-888.726879	-4.537254	1.186138
-891.973109	-11.491074	1.191142
-895.841056	-1.601898	1.196147
-899.711833	-5.555926	1.201152
-902.881948	-13.892230	1.206157
-907.105357	-8.072970	1.211162
-910.323397	-5.762216	1.216166
-914.580294	-3.752124	1.221171
-918.547547	-1.012496	1.226176
-922.032891	-9.421373	1.231181
-926.275796	2.497360	1.236186
-929.614079	-14.846113	1.241190
-933.369298	-11.713023	1.246195
-937.136629	0.178569	1.251200
-940.875989	-6.956522	1.256205
-944.794026	2.995933	1.261210
-948.476847	-7.708840	1.266214
-952.138432	-11.382424	1.271219
-955.943311	-8.859504	1.276224
-959.710196	-11.267328	1.281229
-963.593788	-3.818173	1.286234
-966.963514	-14.721205	1.291238
-970.851788	-3.500910	1.296243
-974.528644	-7.449552	1.301248
-978.725287	-9.284012	1.306253
-982.620834	-4.794343	1.311258
-986.005689	-9.078234	1.316262
-990.267300	-4.600973	1.321267
-993.693755	-4.090717	1.326272
-997.118280	-3.924531	1.331277
-1001.180444	-4.692393	1.336282
-1004.769529	-6.128821	1.341286
-1008.605835	-7.246594	1.346291
-1012.642939	-3.957915	1.351296
-1016.390604	-7.310133	1.356301
-1020.184406	-1.562535	1.361306
-1023.638134	-4.835599	1.366310
-1027.232729	1.827872	1.371315
-1031.219565	-1.858221	1.376320
-1034.841407	-7.234778	1.381325
-1039.145533	-0.460965	1.386330
-1042.726765	-6.058464	1.391334
-1046.217660	-6.946000	1.396339
-1049.767408	-11.173461	1.401344
-1053.667925	-11.675358	1.406349
-1057.739946	-2.057634	1.411354
-1061.128705	-8.337150	1.416358
-1064.876211	1.231836	1.421363
-1068.761435	-4.665494	1.426368
-1072.110346	-14.797431	1.431373
-1076.383486	1.812945	1.436378
-1080.072996	-6.326490	1.441382
-1084.150118	-2.312220	1.446387
-1088.046459	-0.211260	1.451392
-1091.572567	-1.902047	1.456397
-1095.343891	-2.402464	1.461402
-1098.619495	-10.406231	1.466406
-1102.296438	-0.034796	1.471411
-1106.625707	-5.288612	1.476416
-1109.998132	-6.286464	1.481421
-1114.350051	-7.282157	1.486426
-1117.945545	-11.171043	1.491430
-1121.401425	-2.236811	1.496435
-1125.340787	-9.962472	1.501440
-1128.899679	-4.255439	1.506445
-1132.983029	-0.585430	1.511450
-1136.330677	-11.245734	1.516454
-1140.167763	-6.314168	1.521459
-1144.078702	-2.605494	1.526464
-1147.740445	-7.157073	1.531469
-1152.066531	-0.234471	1.536474
-1155.427012	-7.731005	1.541478
-1159.101231	-5.055204	1.546483
-1162.987039	-3.204956	1.551488
-1166.310559	-11.445375	1.556493
-1170.188315	-0.748408	1.561498
-1174.273269	-9.660172	1.566502
-1178.097860	-3.631444	1.571507
-1181.778589	2.607657	1.576512
-1185.107995	1.607761	1.581517
-1189.273340	3.198437	1.586522
-1192.956491	-11.968497	1.591526
-1196.552085	-15.936086	1.596531
-1200.419235	-7.713354	1.601536
-1204.372658	-7.408620	1.606541
-1208.352547	0.308637	1.611546
-1211.487046	-13.662455	1.616550
-1215.263012	-10.180260	1.621555
-1219.527227	-5.803096	1.626560
-1223.014224	-5.136165	1.631565
-1227.362709	0.706825	1.636570
-1230.841917	3.296342	1.641574
-1234.175986	-2.048676	1.646579
-1237.956527	-7.639198	1.651584
-1241.458048	-8.531046	1.656589
-1245.711307	-1.138977	1.661594
-1249.397100	-4.904399	1.666598
-1253.375652	-1.908522	1.671603
-1256.758447	1.759972	1.676608
-1260.301578	-13.184831	1.681613
-1264.309991	-5.798800	1.686618
-1268.045519	-10.048223	1.691622
-1272.227892	0.845882	1.696627
-1276.047573	6.411951	1.701632
-1279.732767	-0.551474	1.706637
-1283.385288	-4.525586	1.711642
-1287.063215	-8.782620	1.716646
-1290.695772	-1.306892	1.721651
-1294.345072	-2.373698	1.726656
-1297.844278	1.712442	1.731661
-1301.980615	0.338834	1.736666
-1305.579786	-11.693851	1.741670
-1309.678964	-8.144005	1.746675
-1313.550950	-7.967233	1.751680
-1317.017241	-15.221082	1.756685
-1321.042812	-2.188490	1.761690
-1324.420943	-14.967702	1.766694
-1328.569345	-7.667965	1.771699
-1332.285298	-10.673087	1.776704
-1335.310399	-17.795682	1.781709
-1339.633468	-16.548487	1.786714
-1343.490157	-18.673230	1.791718
-1347.581921	-11.084494	1.796723
-1350.937571	-13.043431	1.801728
-1354.322991	-13.542121	1.806733
-1358.549592	-15.162941	1.811738
-1362.042164	-28.120872	1.816742
-1365.867570	-14.566771	1.821747
-1369.702932	-16.150854	1.826752
-1373.568632	-15.366305	1.831757
-1377.427196	-20.348027	1.836762
-1380.880542	-18.973489	1.841766
-1384.530646	-16.022088	1.846771
-1388.440508	-19.361914	1.851776
-1392.217245	-23.604529	1.856781
-1396.432715	-10.952993	1.861786
-1399.766423	-13.759011	1.866790
-1403.598510	-15.067604	1.871795
-1407.377690	-22.203408	1.876800
-1410.840341	-11.544147	1.881805
-1414.859566	-12.032736	1.886810
-1418.493056	-18.151096	1.891814
-1422.167919	-18.551308	1.896819
-1426.265454	-15.305864	1.901824
-1430.159586	-25.895547	1.906829
-1434.063824	-8.832740	1.911834
-1437.476014	-17.591534	1.916838
-1441.207131	-20.627162	1.921843
-1445.017970	-9.648761	1.926848
-1448.715389	-17.213888	1.931853
-1452.650585	-13.123945	1.936858
-1456.088581	-19.675652	1.941862
-1460.278065	-17.587060	1.946867
-1463.781604	-18.076137	1.951872
-1467.262812	-23.086586	1.956877
-1471.210161	-17.914495	1.961882
-1475.062710	-17.671180	1.966886
-1478.735968	-11.880668	1.971891
-1482.653758	-7.198971	1.976896
-1486.162168	-17.569636	1.981901
-1490.015690	-17.576867	1.986906
-1493.658052	-17.833941	1.991910
-1497.504969	-6.840219	1.996915
-1501.936459	-9.347504	2.006912
-1502.560599	-14.501888	2.016909
-1499.948063	-12.160019	2.026906
-1497.276531	-9.110766	2.036902
-1494.637948	-9.572476	2.046899
-1493.375194	-12.734857	2.056896
-1491.412466	-10.852593	2.066893
-1489.514887	-13.611377	2.076890
-1487.320281	-8.973140	2.086886
-1485.455889	-13.662356	2.096883
-1483.603341	-13.745558	2.106880
-1481.542627	-12.891060	2.116877
-1479.843970	-9.644949	2.126874
-1478.150353	-7.241169	2.136870
-1476.241551	-20.613622	2.146867
-1474.156223	-13.071621	2.156864
-1472.149375	-16.744711	2.166861
-1470.429241	-20.292942	2.176858
-1468.519560	-8.050800	2.186854
-1466.531772	-8.256695	2.196851
-1464.471793	-7.075227	2.206848
-1462.846701	-10.031933	2.216845
-1461.150312	-6.610184	2.226842
-1459.198541	-11.685995	2.236838
-1456.994225	-8.776616	2.246835
-1455.264043	-6.546038	2.256832
-1453.522031	-8.817262	2.266829
-1451.747440	-14.175744	2.276826
-1449.564610	-11.365547	2.286822
-1447.776669	-8.877375	2.296819
-1445.859431	-11.203492	2.306816
-1443.702450	-11.662241	2.316813
-1442.165319	-5.058726	2.326810
-1440.281428	-6.621619	2.336806
-1438.217861	-11.432688	2.346803
-1436.717681	-12.019949	2.356800
-1434.612958	-9.729326	2.366797
-1432.720508	-11.918834	2.376794
-1430.898427	-13.324984	2.386790
-1428.783656	-12.720667	2.396787
-1427.173034	-6.432059	2.406784
-1425.097853	-10.253417	2.416781
-1423.342972	-9.473056	2.426778
-1421.425873	-4.932425	2.436774
-1419.459914	-11.084140	2.446771
-1417.789940	-9.338094	2.456768
-1415.763680	-8.178027	2.466765
-1413.861039	-9.548115	2.476762
-1412.181449	-10.085139	2.486758
-1410.205395	-11.836444	2.496755
-1408.252339	-6.690517	2.506752
-1406.583541	-13.888835	2.516749
-1404.131272	-11.540143	2.526746
-1402.672872	-4.196112	2.536742
-1400.677523	-11.824068	2.546739
-1398.660759	-9.241440	2.556736
-1397.054096	-12.187256	2.566733
-1395.277904	-7.791409	2.576730
-1393.095129	-13.129935	2.586726
-1391.326276	-10.921288	2.596723
-1389.393009	-13.080981	2.606720
-1387.809133	-15.407365	2.616717
-1385.673287	-13.967978	2.626714
-1383.903971	-13.518313	2.636710
-1382.022966	-9.369757	2.646707
-1379.827984	-7.283001	2.656704
-1378.147748	-5.666461	2.666701
-1376.477315	-1.337349	2.676698
-1374.234309	-4.898168	2.686694
-1372.410832	-4.684527	2.696691
-1370.783871	-8.647241	2.706688
-1368.973181	-3.593749	2.716685
-1366.896756	-5.391085	2.726682
-1365.053911	-5.134750	2.736678
-1363.067170	-6.112479	2.746675
-1361.290458	-10.291786	2.756672
-1359.394268	-4.276201	2.766669
-1357.498129	-4.228914	2.776666
-1355.966645	-8.147915	2.786662
-1353.817068	-1.110274	2.796659
-1351.781136	-6.932092	2.806656
-1349.817786	-2.593006	2.816653
-1348.180303	-8.655771	2.826650
-1346.092792	-1.148723	2.836646
-1344.938934	-3.876765	2.846643
-1342.297654	-9.601265	2.856640
-1340.864255	-4.683143	2.866637
-1338.835905	-9.659014	2.876634
-1336.826932	-9.583983	2.886630
-1334.867467	-6.308454	2.896627
-1333.086299	-10.540558	2.906624
-1331.240579	-2.919005	2.916621
-1329.520102	2.058964	2.926618
-1327.455561	-0.224322	2.936614
-1325.573709	-4.589378	2.946611
-1323.548491	-5.660072	2.956608
-1321.695779	-2.327970	2.966605
-1320.177818	-9.453146	2.976602
-1318.323234	-1.572478	2.986598
-1316.241059	-4.711192	2.996595
-1314.262026	-6.229214	3.006592
-1312.465344	-7.939097	3.016589
-1310.631039	-2.049350	3.026586
-1308.631504	-5.260092	3.036582
-1306.693104	-5.941093	3.046579
-1305.065027	-5.422972	3.056576
-1303.304906	-6.358063	3.066573
-1300.829230	1.382163	3.076570
-1299.204164	-4.384906	3.086566
-1297.882059	-5.527778	3.096563
-1295.839719	-7.491698	3.106560
-1293.587545	-4.468240	3.116557
-1291.925975	-2.046557	3.126554
-1290.162881	-5.988375	3.136550
-1287.875530	-3.714211	3.146547
-1286.033903	-12.024830	3.156544
-1284.380477	-6.857679	3.166541
-1282.365600	1.441044	3.176538
-1280.739799	-1.420920	3.186534
-1278.686723	-4.605470	3.196531
-1276.849849	-6.727540	3.206528
-1274.724341	-8.671595	3.216525
-1273.232487	-7.061143	3.226522
-1271.235641	-11.381403	3.236518
-1269.178441	-9.610378	3.246515
-1267.563645	-7.724340	3.256512
-1265.396968	-7.218178	3.266509
-1264.002687	-5.058430	3.276506
-1261.923537	-4.678781	3.286502
-1259.623949	-9.192741	3.296499
-1258.077769	-10.403028	3.306496
-1256.323787	-8.346629	3.316493
-1254.376073	-3.627594	3.326490
-1252.084904	-6.144447	3.336486
-1250.510747	-3.290331	3.346483
-1248.759535	-10.282268	3.356480
-1246.930458	-10.893621	3.366477
-1244.996939	-0.290831	3.376474
-1242.912627	-3.595611	3.386470
-1241.012813	-8.868196	3.396467
-1239.219910	-6.912747	3.406464
-1237.361236	-8.275657	3.416461
-1235.609782	-5.604637	3.426458
-1233.749880	-8.747183	3.436454
-1231.998417	-8.450857	3.446451
-1229.736732	-7.119879	3.456448
-1227.921210	-7.495368	3.466445
-1226.078994	-3.171524	3.476442
-1224.237137	-6.795904	3.486438
-1222.298371	-4.829046	3.496435
-1220.649049	-8.012095	3.506432
-1218.797819	-1.335518	3.516429
-1216.739541	-4.764001	3.526426
-1214.801361	-7.829060	3.536422
-1213.185056	-9.601582	3.546419
-1211.236256	-5.509515	3.556416
-1209.002731	-4.833999	3.566413
-1207.406807	-6.094844	3.576410
-1205.505981	-5.988183	3.586406
-1203.815968	-8.307747	3.596403
-1201.475485	-4.887807	3.606400
-1199.678885	-7.672836	3.616397
-1198.089780	-5.738428	3.626394
-1196.192279	-6.477529	3.636390
-1194.338406	-9.352243	3.646387
-1192.650568	-4.490521	3.656384
-1190.480744	0.532501	3.666381
-1188.691278	1.478032	3.676378
-1186.491251	-0.136821	3.686374
-1184.669115	-2.265937	3.696371
-1182.865064	-6.222126	3.706368
-1181.314937	-10.756622	3.716365
-1179.342541	-3.857823	3.726362
-1177.429516	-4.517290	3.736358
-1175.390134	3.419202	3.746355
-1173.473085	-3.245543	3.756352
-1171.540018	-7.304470	3.766349
-1170.021230	-4.390913	3.776346
-1168.000274	-9.818612	3.786342
-1166.167959	-8.669923	3.796339
-1164.316936	-16.312496	3.806336
-1162.341323	-7.784753	3.816333
-1160.250846	-11.028868	3.826330
-1158.859606	-6.143352	3.836326
-1156.659193	-8.770327	3.846323
-1154.540010	-1.696045	3.856320
-1152.776740	-10.292452	3.866317
-1151.369649	-9.781498	3.876314
-1149.098014	-10.340422	3.886310
-1147.033641	-9.074110	3.896307
-1145.694482	-10.443832	3.906304
-1143.808506	-9.595811	3.916301
-1141.578889	-8.496454	3.926298
-1139.810306	-5.349686	3.936294
-1137.719798	-3.193876	3.946291
-1136.085130	-3.226155	3.956288
-1134.439998	-15.422535	3.966285
-1132.154999	-12.587322	3.976282
-1130.412684	-4.818001	3.986278
-1128.536636	-6.879910	3.996275
-1126.738054	-7.427870	4.006272
-1124.632819	0.806024	4.016269
-1122.959166	-5.576591	4.026266
-1121.093268	-7.951075	4.036262
-1119.281880	-5.779018	4.046259
-1117.176119	-6.693474	4.056256
-1115.296739	-7.404349	4.066253
-1113.526838	-3.253576	4.076250
-1111.717406	-1.611717	4.086246
-1109.779019	-1.312043	4.096243
-1107.761750	-5.787015	4.106240
-1105.971485	-7.925182	4.116237
-1104.279633	-4.898741	4.126234
-1102.170209	-2.441192	4.136230
-1100.253645	-1.798551	4.146227
-1098.639683	-0.228042	4.156224
-1096.599595	-2.398271	4.166221
-1094.867696	-8.605450	4.176218
-1093.102475	-5.469160	4.186214
-1091.141533	-5.959381	4.196211
-1089.128472	-3.606404	4.206208
-1087.213125	-3.260395	4.216205
-1085.451784	-3.844998	4.226202
-1083.406194	-5.485577	4.236198
-1081.713588	-9.243868	4.246195
-1079.781194	-6.484829	4.256192
-1077.841312	-10.145304	4.266189
-1076.061492	-9.237617	4.276186
-1074.276932	-6.930181	4.286182
-1072.300615	-11.963827	4.296179
-1070.114117	-11.959591	4.306176
-1068.462690	-11.642404	4.316173
-1066.672487	-5.516452	4.326170
-1064.813677	-4.433498	4.336166
-1062.919783	-5.198757	4.346163
-1061.124896	-8.491822	4.356160
-1059.035436	-6.425772	4.366157
-1057.225457	-9.307570	4.376154
-1055.378899	-8.980532	4.386150
-1053.441783	-1.777557	4.396147
-1051.723601	-9.496699	4.406144
-1049.437593	-7.132082	4.416141
-1048.134335	-8.687057	4.426138
-1046.062093	-4.622482	4.436134
-1044.265149	-7.004826	4.446131
-1042.385719	-4.920957	4.456128
-1040.199668	-5.895554	4.466125
-1038.688406	-6.263285	4.476122
-1036.226065	-8.221527	4.486118
-1034.894053	-1.859636	4.496115
-1032.743472	-6.276923	4.506112
-1030.864807	-12.542266	4.516109
-1029.174938	-4.980785	4.526106
-1027.371720	-3.074184	4.536102
-1025.340295	-12.348121	4.546099
-1023.528435	-8.802400	4.556096
-1021.446666	-12.453944	4.566093
-1019.696891	-6.330962	4.576090
-1018.254570	-5.659774	4.586086
-1016.036545	-1.940586	4.596083
-1014.060928	-13.078192	4.606080
-1012.257114	-10.527475	4.616077
-1010.304784	-15.599865	4.626074
-1008.378331	-8.286202	4.636070
-1006.559042	-4.634287	4.646067
-1004.643438	-5.218237	4.656064
-1002.914543	-1.300814	4.666061
-1000.888280	-3.380331	4.676058
-999.121332	-8.189387	4.686054
-997.187689	-5.403634	4.696051
-995.263123	-2.253276	4.706048
-993.487644	-6.435281	4.716045
-991.722257	-6.281524	4.726042
-989.694907	-4.851257	4.736038
-988.060344	-3.034495	4.746035
-985.831329	-7.833751	4.756032
-984.120563	-5.369183	4.766029
-982.228912	-4.566147	4.776026
-980.311871	-5.546617	4.786022
-978.463778	-2.175596	4.796019
-976.481758	-2.585410	4.806016
-974.483314	-4.624141	4.816013
-972.658993	-4.192430	4.826010
-970.908815	-6.205668	4.836006
-969.282500	-1.296039	4.846003
-967.255819	-9.299719	4.856000
-965.369403	-6.290075	4.865997
-963.441497	-6.244389	4.875994
-961.612040	-3.580891	4.885990
-959.747776	-2.306095	4.895987
-957.612303	-5.108818	4.905984
-955.808042	-6.898591	4.915981
-954.011156	-2.363589	4.925978
-952.332446	-8.096385	4.935974
-950.327196	-8.874623	4.945971
-948.411001	-7.841803	4.955968
-946.649334	-5.983758	4.965965
-944.508776	-3.938404	4.975962
-942.632391	-1.099239	4.985958
-941.403526	-0.674921	4.995955
-938.965512	-3.221270	5.005952
-937.221626	-2.326677	5.015949
-935.134938	3.384092	5.025946
-933.707726	1.528309	5.035942
-931.472496	-1.462445	5.045939
-929.361226	6.248057	5.055936
-927.688172	-2.640093	5.065933
-925.944813	-1.933299	5.075930
-924.186063	-1.292121	5.085926
-922.181976	-4.522221	5.095923
-920.389014	-0.648133	5.105920
-918.135410	-1.794470	5.115917
-916.321431	-4.015235	5.125914
-914.905960	-7.312266	5.135910
-912.816774	-4.829202	5.145907
-910.852609	-1.070900	5.155904
-909.053798	-4.593427	5.165901
-907.166411	-1.740202	5.175898
-905.119150	-5.202977	5.185894
-903.432773	0.424983	5.195891
-901.815927	-12.002006	5.205888
-899.658263	-0.503160	5.215885
-897.469820	-3.806924	5.225882
-895.758220	-2.018202	5.235878
-894.080625	-4.894505	5.245875
-892.188521	-1.516239	5.255872
-890.151093	-8.050019	5.265869
-888.557307	0.049564	5.275866
-886.713882	-0.919061	5.285862
-884.363983	-6.490701	5.295859
-882.688969	-2.784041	5.305856
-880.949013	-2.095616	5.315853
-879.017417	-4.470944	5.325850
-876.980689	-4.734686	5.335846
-875.170194	-6.898022	5.345843
-873.545069	-1.986553	5.355840
-871.522702	-7.253190	5.365837
-869.388197	-5.113642	5.375834
-867.778956	1.969817	5.385830
-865.998742	-3.014950	5.395827
-863.882810	-4.380802	5.405824
-862.144109	-2.623229	5.415821
-860.065826	-4.309897	5.425818
-858.592833	-4.564027	5.435814
-856.591652	-3.044198	5.445811
-854.404592	1.763245	5.455808
-852.412953	-4.167931	5.465805
-850.961772	-4.251204	5.475802
-849.130408	-9.349922	5.485798
-846.998127	-9.385759	5.495795
-845.364249	-9.853492	5.505792
-843.159250	-5.034698	5.515789
-841.276697	-10.488957	5.525786
-839.607042	-6.361415	5.535782
-838.045578	-9.463848	5.545779
-835.978497	-5.808774	5.555776
-834.012378	-16.658944	5.565773
-832.000906	-10.579223	5.575770
-830.186025	-9.856948	5.585766
-828.325483	-14.690318	5.595763
-826.376446	-8.040091	5.605760
-824.470449	-14.398072	5.615757
-822.889088	-4.564373	5.625754
-820.720966	-6.873253	5.635750
-819.107491	-7.715071	5.645747
-817.295861	-7.903307	5.655744
-814.869164	-8.038280	5.665741
-813.198636	-3.482967	5.675738
-811.523435	0.140035	5.685734
-809.870264	2.929728	5.695731
-807.782328	0.142629	5.705728
-805.674904	-1.543913	5.715725
-803.810289	-4.666361	5.725722
-802.119904	-3.068386	5.735718
-800.392697	-8.301999	5.745715
-798.302909	-6.321025	5.755712
-796.438120	-4.651450	5.765709
-794.516322	-6.139366	5.775706
-792.627334	-10.472001	5.785702
-790.786641	-7.641217	5.795699
-788.990068	-5.201268	5.805696
-787.034662	-8.510317	5.815693
-785.058726	-9.848986	5.825690
-783.354961	-6.127900	5.835686
-781.486798	-6.792508	5.845683
-779.529746	-6.302914	5.855680
-777.756946	-6.751752	5.865677
-775.675419	-8.819387	5.875674
-773.909831	-9.270228	5.885670
-772.120662	-5.038579	5.895667
-770.174291	-6.500404	5.905664
-768.289917	-8.189158	5.915661
-766.370154	-10.845133	5.925658
-764.467347	-9.789496	5.935654
-762.886399	-4.315102	5.945651
-760.612597	-9.809728	5.955648
-758.876163	-8.596445	5.965645
-756.964978	-9.053174	5.975642
-754.963078	-9.871764	5.985638
-753.406889	-7.083901	5.995635
-751.697110	-2.043767	6.005632
-749.416239	-10.605790	6.015629
-747.484069	-4.710680	6.025626
-745.618156	-4.841222	6.035622
-744.162194	-0.535772	6.045619
-742.175209	-9.044507	6.055616
-740.274429	-11.714796	6.065613
-737.978044	-11.656762	6.075610
-736.332966	-13.515667	6.085606
-734.303007	-7.405650	6.095603
-733.057130	-4.006082	6.105600
-731.045209	-5.978872	6.115597
-728.718019	-7.061001	6.125594
-726.995031	-19.084856	6.135590
-725.302108	-7.551038	6.145587
-723.170323	-3.694624	6.155584
-721.409477	-12.996142	6.165581
-719.461037	-7.853599	6.175578
-717.578731	-5.275718	6.185574
-715.578669	-7.270283	6.195571
-713.972278	-10.051401	6.205568
-712.017255	-7.366716	6.215565
-709.847262	-8.433180	6.225562
-708.270739	-13.587387	6.235558
-706.636551	-14.280862	6.245555
-704.482722	-11.525310	6.255552
-702.747221	-10.190259	6.265549
-700.866190	-13.875770	6.275546
-698.631637	-9.645761	6.285542
-696.908948	-12.036509	6.295539
-695.109209	-11.166448	6.305536
-693.520427	-10.137942	6.315533
-691.461086	-7.116229	6.325530
-689.258215	-13.396814	6.335526
-687.597819	-9.359256	6.345523
-685.741029	-11.482480	6.355520
-683.654714	-13.636062	6.365517
-681.764016	-8.282157	6.375514
-680.345605	-9.642180	6.385510
-678.333395	-7.122918	6.395507
-676.494989	-3.227476	6.405504
-674.301057	-9.042416	6.415501
-672.663188	-8.533312	6.425498
-670.799331	-13.689197	6.435494
-669.095077	-14.518577	6.445491
-666.772809	-8.886252	6.455488
-665.104006	-14.694644	6.465485
-663.113523	-13.177676	6.475482
-661.222713	-9.983747	6.485478
-659.483584	-10.806060	6.495475
-657.571511	-14.032294	6.505472
-655.516739	-17.905002	6.515469
-653.874446	-15.163986	6.525466
-652.141190	-22.858432	6.535462
-650.148285	-11.235117	6.545459
-648.215769	-10.935703	6.555456
-646.304007	-15.884489	6.565453
-644.470892	-19.194411	6.575450
-642.506047	-22.435378	6.585446
-640.779383	-19.909937	6.595443
-638.929948	-15.986231	6.605440
-636.877434	-17.210699	6.615437
-634.877875	-17.758817	6.625434
-633.193096	-20.201883	6.635430
-631.358141	-17.442686	6.645427
-629.362942	-16.153808	6.655424
-627.697376	-18.770641	6.665421
-626.087963	-12.214395	6.675418
-623.699011	-10.898421	6.685414
-621.768478	-10.663404	6.695411
-620.067754	-14.956357	6.705408
-618.276983	-12.336930	6.715405
-616.191904	-12.181862	6.725402
-614.373440	-9.791063	6.735398
-612.782368	-9.489175	6.745395
-610.771694	-9.161165	6.755392
-608.671981	-10.167362	6.765389
-606.743947	-8.255110	6.775386
-605.145542	-7.895968	6.785382
-603.112910	-10.029853	6.795379
-601.195230	-14.354295	6.805376
-599.560160	-14.315214	6.815373
-597.988447	-10.130792	6.825370
-595.552846	-14.995859	6.835366
-593.774541	-15.023866	6.845363
-591.754984	-15.451987	6.855360
-590.065885	-15.006272	6.865357
-588.388897	-19.456462	6.875354
-586.212969	-15.316450	6.885350
-584.296989	-11.782272	6.895347
-582.486027	-12.044432	6.905344
-580.752712	-8.569490	6.915341
-578.697207	-11.692261	6.925338
-576.701070	-17.936565	6.935334
-575.116316	-15.933135	6.945331
-573.275580	-13.323234	6.955328
-571.409894	-20.293528	6.965325
-569.255191	-15.419066	6.975322
-567.456830	-18.323910	6.985318
-565.502137	-19.104801	6.995315
-563.944942	-11.899122	7.005312
-562.068994	-17.056859	7.015309
-559.983464	-10.076096	7.025306
-558.227710	-8.276808	7.035302
-556.212741	-13.163068	7.045299
-554.289825	-14.557815	7.055296
-552.546949	-17.640100	7.065293
-550.594489	-13.469095	7.075290
-548.586522	-18.594226	7.085286
-546.936067	-20.018077	7.095283
-545.227573	-16.202832	7.105280
-542.878159	-12.756799	7.115277
-541.429026	-9.316960	7.125274
-539.434467	-2.490588	7.135270
-537.401047	-9.148185	7.145267
-535.778138	-5.390312	7.155264
-533.947779	-8.267087	7.165261
-531.653663	-7.750600	7.175258
-529.881581	-5.590744	7.185254
-528.245885	-6.352233	7.195251
-526.222330	-11.280893	7.205248
-524.407710	-10.943599	7.215245
-522.105124	-15.648404	7.225242
-520.902376	-17.324410	7.235238
-518.829267	-12.575812	7.245235
-516.839988	-8.251185	7.255232
-515.249885	-12.010090	7.265229
-512.947857	-13.170096	7.275226
-511.301948	-14.370568	7.285222
-509.208123	-15.031531	7.295219
-507.887932	-8.124268	7.305216
-505.579122	-8.326938	7.315213
-503.483110	-7.256157	7.325210
-501.775645	-12.042735	7.335206
-499.871354	-12.185530	7.345203
-498.284908	-8.860750	7.355200
-496.508488	-8.901015	7.365197
-494.269678	-14.307707	7.375194
-492.592392	-16.097382	7.385190
-490.294269	-9.502607	7.395187
-488.844322	-8.851258	7.405184
-486.822965	-13.190593	7.415181
-485.265637	-7.194337	7.425178
-482.922707	-8.207690	7.435174
-481.214336	-11.502308	7.445171
-479.439343	-7.797104	7.455168
-477.470328	-4.958139	7.465165
-475.472278	-6.824293	7.475162
-473.557125	-13.028745	7.485158
-471.763055	-15.994414	7.495155
-469.958071	-15.840276	7.505152
-468.113414	-16.894039	7.515149
-466.278657	-13.943626	7.525146
-464.214195	-10.706214	7.535142
-462.383840	-14.492400	7.545139
-460.601579	-16.502500	7.555136
-458.819528	-19.382556	7.565133
-456.742972	-24.475935	7.575130
-454.914137	-17.215664	7.585126
-453.027829	-13.596111	7.595123
-450.986225	-7.291905	7.605120
-449.424541	-9.691507	7.615117
-447.653660	-11.360310	7.625114
-445.368559	-14.484898	7.635110
-443.477394	-15.558701	7.645107
-441.821139	-16.375518	7.655104
-440.309610	-13.758729	7.665101
-438.195154	-9.589811	7.675098
-436.070301	-11.308814	7.685094
-434.164171	-15.225500	7.695091
-432.471951	-13.927547	7.705088
-430.519626	-16.608986	7.715085
-428.635962	-7.216410	7.725082
-426.727220	-13.697696	7.735078
-424.882248	-10.614672	7.745075
-423.207424	-3.629772	7.755072
-421.316523	-11.173986	7.765069
-419.349969	-11.850865	7.775066
-417.253023	-14.983278	7.785062
-415.408128	-14.031794	7.795059
-413.662320	-10.130828	7.805056
-411.851790	-7.334395	7.815053
-410.004508	-8.656953	7.825050
-407.778950	-12.575677	7.835046
-406.270740	-12.915677	7.845043
-404.403316	-13.961975	7.855040
-402.229205	-7.268359	7.865037
-400.596087	-13.947194	7.875034
-398.670069	-10.397093	7.885030
-396.595729	-11.899578	7.895027
-394.936722	-6.162647	7.905024
-393.079702	-13.284592	7.915021
-391.084070	-20.556559	7.925018
-388.864631	-13.486490	7.935014
-387.693608	-16.755247	7.945011
-385.690677	-14.101619	7.955008
-383.881814	-11.870158	7.965005
-381.727001	-13.454951	7.975002
-379.903849	-5.791075	7.984998
-377.859041	-6.273574	7.994995
-376.132656	-8.991529	8.004992
-374.538486	-7.704721	8.014989
-372.510526	-2.165624	8.024986
-370.446259	-4.954890	8.034982
-368.501452	-7.102980	8.044979
-366.780275	-10.333251	8.054976
-364.817907	-4.641572	8.064973
-362.727905	-5.736006	8.074970
-361.130613	-13.838033	8.084966
-359.726330	-6.855681	8.094963
-357.545734	-11.305600	8.104960
-355.268105	-9.294217	8.114957
-353.447863	-6.475605	8.124954
-351.681462	-14.099366	8.134950
-349.827588	-8.155094	8.144947
-347.925608	-11.229481	8.154944
-346.173832	-5.172589	8.164941
-344.220748	-5.807783	8.174938
-342.236783	-12.681541	8.184934
-340.330156	-12.807213	8.194931
-338.582040	-8.415509	8.204928
-336.857087	-10.629527	8.214925
-334.678393	-10.388106	8.224922
-333.347416	-8.523994	8.234918
-331.088760	-17.634735	8.244915
-329.347786	-10.826114	8.254912
-326.974160	-14.788930	8.264909
-325.533390	-14.650749	8.274906
-323.807500	-14.338612	8.284902
-321.626943	-20.272690	8.294899
-319.882395	-10.092027	8.304896
-318.137942	-9.553903	8.314893
-316.260672	-2.725973	8.324890
-314.255958	-6.014103	8.334886
-312.269030	-4.406268	8.344883
-310.214442	-7.042361	8.354880
-308.540911	-3.216615	8.364877
-306.678507	-8.034116	8.374874
-305.051046	-8.009408	8.384870
-302.965542	-10.655166	8.394867
-301.077945	-5.635175	8.404864
-299.271283	-9.332200	8.414861
-297.278950	-11.884134	8.424858
-295.736423	-10.701134	8.434854
-293.460805	-8.912000	8.444851
-291.563959	-9.100809	8.454848
-289.809434	-10.967412	8.464845
-287.892077	-10.223184	8.474842
-286.292478	-10.609276	8.484838
-284.397643	-12.504588	8.494835
-282.064263	-11.967286	8.504832
-280.277482	-12.162202	8.514829
-278.591665	-9.173654	8.524826
-277.031272	-11.389785	8.534822
-274.742744	-13.928979	8.544819
-272.907041	-9.492783	8.554816
-271.047574	-10.316658	8.564813
-269.552326	-10.720820	8.574810
-267.271468	-10.037753	8.584807
-265.137479	-15.219094	8.594803
-263.605103	-11.590260	8.604800
-261.936533	-9.165785	8.614797
-259.890674	-7.201000	8.624794
-257.672204	-6.313756	8.634791
-255.920766	-11.411927	8.644787
-254.323013	-14.548210	8.654784
-252.628456	-14.466282	8.664781
-250.488444	-16.127544	8.674778
-248.089935	-13.851144	8.684775
-246.694234	-17.807798	8.694771
-245.042615	-9.026967	8.704768
-242.965601	-5.955567	8.714765
-240.840628	-12.845439	8.724762
-239.138957	-13.448317	8.734759
-237.374022	-12.821825	8.744755
-235.223986	-10.864172	8.754752
-233.607708	-15.885491	8.764749
-231.727325	-10.695346	8.774746
-229.940469	-3.815018	8.784743
-227.733487	-8.095355	8.794739
-225.727019	-25.493067	8.804736
-224.185043	-22.192581	8.814733
-222.457475	-18.702240	8.824730
-220.229960	-10.897505	8.834727
-218.416491	-15.841340	8.844723
-216.640247	-19.637660	8.854720
-214.993457	-16.477050	8.864717
-212.834366	-12.937149	8.874714
-210.923206	-17.061311	8.884711
-209.035643	-13.653334	8.894707
-207.148336	-12.272670	8.904704
-205.315631	-15.367472	8.914701
-203.736891	-13.335986	8.924698
-201.598850	-12.025332	8.934695
-199.585903	-15.287840	8.944691
-198.273261	-11.816526	8.954688
-196.336994	-14.335747	8.964685
-194.069660	-13.342559	8.974682
-192.348706	-20.120546	8.984679
-190.623293	-21.328752	8.994675
-188.387684	-23.734684	9.004672
-186.640915	-15.437939	9.014669
-184.612662	-12.046078	9.024666
-182.993540	-20.429377	9.034663
-180.829711	-17.120728	9.044659
-178.951046	-24.152817	9.054656
-177.479188	-14.558519	9.064653
-175.493626	-16.327700	9.074650
-173.537318	-16.743798	9.084647
-171.632731	-16.186911	9.094643
-169.744995	-14.638919	9.104640
-167.934469	-12.835447	9.114637
-166.102293	-14.295936	9.124634
-164.103359	-16.395661	9.134631
-162.151943	-14.060460	9.144627
-160.474714	-15.414114	9.154624
-158.501168	-21.941860	9.164621
-156.580365	-13.661808	9.174618
-154.548955	-18.034062	9.184615
-153.121175	-14.996354	9.194611
-151.133325	-19.672705	9.204608
-149.028402	-18.513034	9.214605
-147.189064	-11.985225	9.224602
-145.486785	-16.581269	9.234599
-143.529369	-15.538581	9.244595
-141.533223	-17.811526	9.254592
-139.916437	-16.933956	9.264589
-138.011478	-18.658667	9.274586
-135.915901	-19.002221	9.284583
-133.831586	-18.215036	9.294579
-132.029936	-16.964329	9.304576
-130.548158	-12.992597	9.314573
-128.389828	-16.020879	9.324570
-126.477620	-12.490452	9.334567
-124.706364	-10.529103	9.344563
-123.013501	-10.254183	9.354560
-120.895653	-7.091296	9.364557
-118.988201	-7.254820	9.374554
-116.939043	-9.356205	9.384551
-115.843865	-10.831697	9.394547
-113.616621	-2.319442	9.404544
-111.463419	-10.683709	9.414541
-109.591800	-4.306278	9.424538
-107.858010	-9.178904	9.434535
-105.701171	-8.152213	9.444531
-104.159403	-12.229993	9.454528
-102.503840	-5.458087	9.464525
-100.482606	-2.983973	9.474522
-98.599251	-11.692016	9.484519
-96.182186	-12.399458	9.494515
-94.557896	-3.596777	9.504512
-92.907198	-1.568800	9.514509
-90.968605	-5.253570	9.524506
-89.387361	-8.616064	9.534503
-87.251208	-17.606006	9.544499
-85.412314	-15.238579	9.554496
-83.421473	-17.973260	9.564493
-81.699434	-5.748815	9.574490
-79.770059	-11.206834	9.584487
-77.611728	-14.203494	9.594483
-75.885146	-9.975519	9.604480
-73.971422	-8.812120	9.614477
-72.002334	-4.157041	9.624474
-70.590763	-3.489841	9.634471
-68.336253	-11.751814	9.644467
-66.452037	-5.076358	9.654464
-64.753315	-10.080729	9.664461
-62.804025	-9.661939	9.674458
-60.859885	-11.239685	9.684455
-59.095717	-9.498208	9.694451
-57.223168	-12.008736	9.704448
-55.432974	-6.570372	9.714445
-53.542569	-5.300605	9.724442
-51.526899	-9.247113	9.734439
-49.517229	-11.436880	9.744435
-47.697224	-12.868497	9.754432
-46.208153	-14.811003	9.764429
-43.696431	-4.918277	9.774426
-42.197441	-8.288147	9.784423
-40.279793	-13.557950	9.794419
-38.162406	-6.442827	9.804416
-36.490805	-6.713925	9.814413
-34.934985	-5.014983	9.824410
-33.309631	-4.056602	9.834407
-31.120674	-10.465463	9.844403
-28.685946	-15.137217	9.854400
-26.916365	-13.560789	9.864397
-25.432964	-13.940806	9.874394
-23.399381	-13.614378	9.884391
-21.371281	-16.007587	9.894387
-19.630110	-11.845054	9.904384
-17.616288	-10.975471	9.914381
-16.014026	-11.622336	9.924378
-14.355265	-6.780340	9.934375
-12.146992	-9.983858	9.944371
-10.441480	-18.063472	9.954368
-8.407784	-12.633913	9.964365
-6.729356	-15.293439	9.974362
-5.121101	7.177611	9.984359
-3.880681	40.572097	9.994355
-2.396018	75.595075	10.004352
-0.842252	137.630943	10.014349
0.000000	188.748398	10.019354
1.007761	224.274079	10.024359
1.306917	257.922761	10.029363
1.697817	291.463847	10.034368
2.651456	308.221579	10.039373
2.678398	326.562176	10.044378
2.912359	352.057563	10.049383
3.163394	363.975771	10.054387
3.143870	378.968069	10.059392
3.527034	370.154950	10.064397
3.522358	384.777454	10.069402
3.675457	386.517804	10.074407
4.344279	393.551771	10.079411
3.876795	390.313278	10.084416
4.159905	381.907198	10.089421
3.948203	386.922744	10.094426
4.048670	393.429195	10.099431
4.084928	396.426101	10.104435
4.200269	403.751783	10.109440
4.264905	405.545670	10.114445
3.997921	394.756218	10.119450
4.420932	406.700648	10.124455
4.556863	414.787881	10.129459
4.334906	416.901874	10.134464
4.466995	408.685450	10.139469
4.255709	413.070151	10.144474
4.562538	421.584295	10.149479
4.546453	423.991885	10.154483
4.429572	425.467794	10.159488
4.950218	430.841211	10.164493
4.606489	430.618636	10.169498
4.757421	425.811760	10.174503
5.057023	425.609575	10.179507
5.024513	424.630878	10.184512
4.797616	418.250529	10.189517
4.761429	416.696826	10.194522
4.766452	419.080547	10.199527
4.739984	424.927585	10.204531
4.751472	433.495153	10.209536
5.085142	430.844808	10.214541
5.061940	437.888251	10.219546
4.988995	440.401108	10.224551
5.211666	437.528767	10.229555
5.415219	445.184180	10.234560
5.675185	442.350045	10.239565
5.344623	449.217011	10.244570
5.580874	445.437321	10.249575
5.303335	453.093779	10.254579
5.232043	454.332181	10.259584
5.419867	450.172278	10.264589
5.306836	454.419893	10.269594
5.302337	458.938784	10.274599
5.605973	462.460767	10.279603
5.832047	466.725261	10.284608
5.813520	464.227282	10.289613
5.490370	468.468991	10.294618
5.462437	460.554031	10.299623
5.638737	465.252247	10.304627
5.388114	478.838578	10.309632
6.026449	481.679544	10.314637
6.159307	488.280221	10.319642
6.258025	485.145363	10.324647
5.834100	468.754239	10.329651
5.959171	479.776412	10.334656
6.501748	485.121120	10.339661
6.328469	484.770431	10.344666
6.117235	479.239123	10.349671
6.297678	473.973355	10.354675
6.291682	485.677191	10.359680
6.680529	494.080524	10.364685
6.576776	478.122453	10.369690
6.333205	477.333538	10.374695
6.396958	482.924932	10.379699
6.371312	489.984559	10.384704
6.923718	496.417394	10.389709
6.545775	503.774498	10.394714
6.877805	498.697434	10.399719
7.057171	491.377030	10.404723
6.615989	481.460557	10.409728
6.655724	480.419870	10.414733
6.885187	500.450441	10.419738
6.811592	510.092931	10.424743
6.812951	508.194178	10.429747
6.834039	508.364429	10.434752
6.996404	504.676934	10.439757
7.198568	519.358046	10.444762
7.270592	521.023034	10.449767
7.395719	517.213741	10.454771
6.756176	515.284746	10.459776
7.204776	513.056033	10.464781
7.037671	518.100780	10.469786
7.110962	509.242385	10.474791
7.296769	514.289189	10.479795
6.798648	515.658756	10.484800
7.325274	511.987277	10.489805
7.288981	522.885409	10.494810
7.557868	529.894923	10.499815
7.970939	545.852893	10.504819
7.626082	535.034755	10.509824
7.684713	523.803756	10.514829
7.610844	527.713979	10.519834
7.603905	526.097251	10.524839
7.765930	541.365117	10.529843
8.112793	540.862075	10.534848
8.373935	537.482098	10.539853
7.712889	537.395291	10.544858
7.759024	529.116813	10.549863
7.985892	542.018328	10.554867
8.063869	549.416277	10.559872
8.427260	550.914944	10.564877
8.126658	551.713681	10.569882
8.358857	554.080114	10.574887
8.783276	547.931718	10.579891
8.322465	537.016954	10.584896
8.233447	524.544765	10.589901
8.154494	526.323722	10.594906
8.420871	528.534886	10.599911
8.799671	542.336279	10.604915
8.490829	539.638584	10.609920
8.127015	529.268182	10.614925
8.342990	543.923462	10.619930
8.502485	547.045826	10.624935
8.608661	562.117614	10.629939
8.505024	558.272256	10.634944
8.796601	559.179971	10.639949
8.634169	570.662818	10.644954
8.749305	566.012995	10.649959
8.969518	559.498189	10.654963
8.538330	565.160674	10.659968
8.798985	564.978894	10.664973
8.926584	568.487979	10.669978
9.161487	561.843093	10.674983
9.437406	569.266252	10.679987
9.454879	567.538390	10.684992
9.614583	560.511253	10.689997
9.323134	557.271451	10.695002
9.255682	561.292626	10.700007
9.130815	560.112604	10.705011
9.217910	556.153246	10.710016
9.271046	558.166610	10.715021
9.157918	569.930180	10.720026
9.428180	582.238171	10.725031
9.809234	592.628232	10.730035
9.657819	597.252602	10.735040
9.967407	586.855177	10.740045
9.657585	599.159511	10.745050
9.853330	589.153989	10.750055
9.846253	596.349481	10.755059
9.863895	591.907593	10.760064
9.812847	594.429600	10.765069
9.655452	581.069385	10.770074
9.951480	591.217535	10.775079
10.073776	600.305280	10.780083
9.952019	593.181091	10.785088
10.032256	587.322548	10.790093
10.298218	601.230306	10.795098
10.299846	585.403545	10.800103
10.465155	593.241760	10.805107
10.308374	599.847683	10.810112
10.778105	586.518327	10.815117
10.536868	589.556380	10.820122
10.426044	576.931502	10.825127
10.483451	565.096680	10.830131
10.184707	570.449453	10.835136
10.642159	579.411186	10.840141
10.418664	592.444505	10.845146
10.773770	599.131212	10.850151
11.001860	596.667993	10.855155
10.937751	596.851834	10.860160
10.775232	569.127671	10.865165
10.853565	569.840736	10.870170
10.392660	562.743848	10.875175
11.063877	577.265049	10.880179
10.910009	596.666175	10.885184
11.098944	598.211597	10.890189
10.815082	608.056427	10.895194
10.970227	603.023311	10.900199
11.105706	599.513550	10.905203
11.181836	598.648403	10.910208
11.241851	602.530984	10.915213
11.183477	607.547381	10.920218
11.400834	599.219475	10.925223
11.272500	606.976798	10.930227
10.920238	609.824401	10.935232
11.117805	600.749004	10.940237
11.077088	608.514430	10.945242
10.992133	604.634540	10.950247
11.247011	605.836701	10.955251
11.347185	631.234069	10.960256
11.587306	624.064761	10.965261
11.584827	630.441079	10.970266
11.708384	627.786365	10.975271
11.677734	631.361709	10.980275
11.281572	630.653894	10.985280
11.979643	624.162191	10.990285
11.677387	624.995889	10.995290
11.612735	624.772953	11.000295
11.918766	624.688016	11.005299
11.959408	633.339363	11.010304
12.067510	617.222766	11.015309
11.693021	636.532975	11.020314
12.143413	637.760726	11.025319
12.416755	655.245555	11.030323
12.303027	656.851875	11.035328
12.421157	650.127800	11.040333
12.310948	641.484678	11.045338
12.214777	650.908506	11.050343
12.615922	644.394766	11.055347
12.673141	653.743666	11.060352
12.756692	623.196757	11.065357
12.448963	624.944406	11.070362
12.753411	627.261479	11.075367
12.713925	619.638442	11.080371
12.362612	629.647013	11.085376
12.681087	630.378550	11.090381
12.667973	652.868707	11.095386
12.820867	659.852630	11.100391
12.758876	659.285484	11.105395
12.706842	660.840961	11.110400
13.450317	656.865195	11.115405
13.207481	661.089417	11.120410
13.210290	656.995237	11.125415
13.302348	646.749163	11.130419
13.080794	637.168145	11.135424
13.025838	621.023933	11.140429
13.041916	641.079272	11.145434
13.096494	650.742414	11.150439
13.215578	648.720784	11.155443
13.022417	658.812962	11.160448
13.609229	651.266637	11.165453
13.382512	655.653872	11.170458
13.276772	661.136747	11.175463
13.390735	659.497566	11.180467
13.290122	660.899939	11.185472
13.491046	656.578612	11.190477
13.484690	654.077082	11.195482
13.536757	658.940260	11.200487
13.623401	656.898571	11.205491
13.370155	660.914714	11.210496
13.863704	679.124562	11.215501
13.792202	686.819244	11.220506
13.779976	684.607235	11.225511
14.614702	683.751979	11.230515
14.126948	677.977685	11.235520
13.938500	668.634223	11.240525
14.065408	663.364309	11.245530
14.046126	673.070786	11.250535
14.190980	677.488651	11.255539
14.186899	689.980845	11.260544
14.819288	687.144034	11.265549
14.182514	680.966141	11.270554
13.908616	667.099289	11.275559
13.827271	676.184869	11.280563
14.121668	686.360155	11.285568
14.380489	679.138950	11.290573
14.380975	688.397571	11.295578
14.664623	686.586238	11.300583
14.382774	687.224291	11.305587
14.199211	690.147506	11.310592
14.762159	680.657380	11.315597
14.629214	686.791173	11.320602
14.761526	693.002513	11.325607
14.914706	692.183420	11.330611
15.266851	697.227413	11.335616
15.002223	692.668085	11.340621
14.923253	688.322004	11.345626
15.106302	681.582830	11.350631
15.195949	686.056812	11.355635
14.912632	692.604110	11.360640
14.887766	681.269609	11.365645
15.038453	696.518946	11.370650
15.289310	711.201161	11.375655
15.677130	715.055144	11.380659
15.380044	703.126147	11.385664
15.510570	688.686975	11.390669
15.420370	691.521181	11.395674
15.502864	689.622079	11.400679
15.441810	680.256713	11.405683
14.883062	697.223012	11.410688
15.554742	700.012973	11.415693
15.247284	716.091576	11.420698
15.683738	717.558108	11.425703
16.110417	717.854487	11.430707
16.001735	719.187187	11.435712
16.245341	711.667186	11.440717
15.979057	720.678209	11.445722
15.788201	707.603920	11.450727
15.998776	700.957332	11.455731
16.048808	715.053399	11.460736
15.967048	717.391085	11.465741
16.040483	709.549710	11.470746
16.184577	708.974924	11.475751
16.052302	707.944309	11.480755
16.043777	709.958067	11.485760
16.127467	703.790623	11.490765
16.087567	716.462811	11.495770
16.037384	717.669482	11.500775
16.255139	719.814313	11.505779
15.922147	734.011703	11.510784
16.292863	718.299399	11.515789
16.173350	720.059616	11.520794
15.971381	725.051647	11.525799
16.458479	735.841226	11.530803
16.693578	748.587068	11.535808
16.758082	739.526500	11.540813
16.728415	751.445644	11.545818
16.979220	745.313820	11.550823
16.867376	737.913579	11.555827
16.799705	736.114119	11.560832
17.168032	736.317301	11.565837
17.094184	737.729605	11.570842
17.136637	741.181349	11.575847
17.241211	734.104572	11.580851
16.975393	739.947333	11.585856
17.333181	742.596552	11.590861
17.469120	740.859236	11.595866
17.149603	717.424048	11.600871
17.268571	713.123662	11.605875
16.895175	722.151769	11.610880
17.068432	730.253727	11.615885
17.161721	740.275042	11.620890
17.309623	737.621156	11.625895
17.233287	742.804473	11.630899
17.513085	745.606485	11.635904
17.561089	736.958571	11.640909
17.397160	744.548173	11.645914
17.403689	737.275714	11.650919
17.529180	736.615582	11.655923
17.540536	756.451054	11.660928
18.016223	741.510484	11.665933
17.643153	747.583251	11.670938
17.417543	745.365843	11.675943
17.721418	758.401931	11.680947
17.530904	771.851211	11.685952
18.178591	779.051174	11.690957
18.240143	775.693516	11.695962
18.296975	769.652545	11.700967
18.551973	771.923912	11.705971
18.095956	772.132415	11.710976
18.756570	753.604610	11.715981
18.417078	745.677684	11.720986
18.232785	733.717266	11.725991
18.250980	730.897984	11.730995
18.150127	747.409672	11.736000
18.501074	748.136038	11.741005
18.368288	755.252308	11.746010
18.030211	766.082058	11.751015
18.424670	761.119531	11.756019
18.371406	771.910166	11.761024
18.384170	768.713261	11.766029
18.440318	768.627178	11.771034
18.608380	775.998259	11.776039
18.601988	769.861713	11.781043
18.500548	776.200261	11.786048
18.787658	767.925791	11.791053
18.795663	774.398274	11.796058
19.145231	785.823284	11.801063
19.546496	784.075184	11.806067
19.077143	776.208379	11.811072
19.018531	766.828374	11.816077
18.815113	769.092429	11.821082
19.074958	775.084760	11.826087
19.204600	789.036521	11.831091
18.995223	804.016961	11.836096
19.390796	796.141507	11.841101
19.338112	796.217867	11.846106
19.269275	796.183260	11.851111
19.648385	792.353886	11.856115
19.308122	796.655190	11.861120
19.533247	783.954470	11.866125
19.462022	802.289249	11.871130
19.668656	794.246804	11.876135
19.907500	790.264755	11.881139
19.548704	791.911754	11.886144
20.089837	787.234918	11.891149
19.622372	801.092686	11.896154
20.089641	792.772121	11.901159
20.410673	790.887002	11.906163
19.872478	784.056228	11.911168
19.997452	792.788841	11.916173
20.019651	794.966450	11.921178
20.020378	789.107891	11.926183
20.013791	794.332143	11.931187
19.811244	797.733088	11.936192
19.989772	794.165950	11.941197
20.155111	795.831856	11.946202
19.727255	796.390694	11.951207
20.027986	790.840689	11.956211
20.035982	798.557445	11.961216
20.007992	796.869924	11.966221
20.004537	821.935636	11.971226
20.280088	818.887625	11.976231
20.687469	822.631280	11.981235
20.491026	827.844823	11.986240
20.692309	826.683724	11.991245
20.442192	834.544173	11.996250
20.437710	826.743548	12.001255
20.723648	825.169963	12.006259
20.411840	824.464453	12.011264
20.918989	824.568221	12.016269
20.745200	829.879080	12.021274
20.735857	818.379563	12.026279
21.273069	812.274572	12.031283
21.293454	829.494019	12.036288
21.638414	819.634857	12.041293
21.184714	818.775353	12.046298
21.012182	824.641117	12.051303
21.391913	821.106539	12.056307
20.987850	810.196707	12.061312
20.839214	793.379667	12.066317
20.706665	792.757534	12.071322
20.591548	792.769734	12.076327
21.099595	801.348209	12.081331
20.842314	802.849702	12.086336
20.934511	785.025976	12.091341
20.761379	788.113133	12.096346
20.729342	793.787737	12.101351
20.978494	803.694347	12.106355
20.902156	806.417550	12.111360
20.830964	791.508959	12.116365
20.950501	798.646510	12.121370
21.340354	796.985388	12.126375
21.175649	789.762292	12.131379
20.878473	793.932139	12.136384
21.131576	795.393229	12.141389
21.092337	791.081782	12.146394
21.014142	789.241415	12.151399
20.852229	791.312767	12.156403
21.189393	792.033448	12.161408
21.271184	783.829565	12.166413
21.044556	795.437950	12.171418
21.110717	788.786758	12.176423
21.020150	774.958371	12.181427
20.688950	769.212688	12.186432
20.858874	765.161211	12.191437
20.889472	781.658281	12.196442
20.865585	776.213675	12.201447
20.998254	772.059325	12.206451
20.820456	766.233980	12.211456
20.863990	764.361585	12.216461
20.805714	774.140583	12.221466
20.970566	764.251836	12.226471
21.114285	761.794162	12.231475
20.472725	768.969509	12.236480
20.904278	774.197990	12.241485
21.229566	772.014141	12.246490
21.242229	764.053115	12.251495
20.910018	769.673081	12.256499
20.875351	773.184443	12.261504
21.004672	767.956686	12.266509
20.812047	764.926586	12.271514
20.583681	759.500407	12.276519
20.826403	764.396292	12.281523
20.892248	766.830296	12.286528
21.019738	761.916658	12.291533
21.058913	764.189330	12.296538
20.897211	765.940512	12.301543
21.217415	764.082338	12.306547
20.985728	768.604444	12.311552
21.062762	749.166747	12.316557
21.051154	763.227748	12.321562
20.822965	761.220490	12.326567
21.085853	757.691947	12.331571
21.102167	760.181160	12.336576
20.957127	766.190756	12.341581
20.779294	772.711803	12.346586
20.781009	766.586581	12.351591
21.067080	767.271254	12.356595
20.655023	770.934275	12.361600
20.878047	767.566634	12.366605
20.860424	775.987655	12.371610
21.035574	773.854561	12.376615
21.291355	772.487648	12.381619
20.874831	764.478377	12.386624
20.959289	736.250860	12.391629
20.900502	738.198520	12.396634
20.700476	737.777970	12.401639
20.798615	740.454408	12.406643
20.777657	744.094468	12.411648
20.664506	753.421720	12.416653
20.844990	766.562655	12.421658
20.648511	771.831379	12.426663
20.936433	770.940327	12.431667
21.020163	778.238125	12.436672
20.612297	778.010001	12.441677
20.881025	779.154773	12.446682
21.220560	772.595609	12.451687
21.326992	778.689684	12.456691
20.645335	759.330403	12.461696
21.233902	745.486769	12.466701
20.749158	748.639389	12.471706
20.865879	756.354551	12.476711
20.837103	741.106499	12.481715
21.060089	750.088390	12.486720
21.132113	744.388794	12.491725
20.742488	750.945188	12.496730
20.816956	748.918045	12.501735
20.939959	753.262146	12.506739
20.458681	757.311531	12.511744
21.154443	743.324640	12.516749
20.979179	750.871898	12.521754
20.872571	751.513542	12.526759
20.979044	755.085969	12.531763
20.938474	751.561672	12.536768
21.026964	749.188506	12.541773
21.084480	759.322776	12.546778
21.144725	745.653296	12.551783
21.194598	758.764592	12.556787
20.839530	760.906172	12.561792
21.063154	751.711404	12.566797
21.014678	755.247043	12.571802
20.850004	750.436779	12.576807
21.033005	754.847007	12.581811
20.955829	760.069889	12.586816
21.293052	748.407914	12.591821
20.594005	744.334187	12.596826
20.633703	747.043603	12.601831
20.838149	746.008166	12.606835
20.882565	760.009764	12.611840
20.950326	749.704412	12.616845
21.018315	757.493582	12.621850
20.872173	745.503414	12.626855
20.996317	748.118934	12.631859
20.836881	743.978065	12.636864
21.033757	744.576035	12.641869
20.715637	730.075910	12.646874
20.658674	730.490432	12.651879
21.205043	738.783628	12.656883
20.510284	744.196473	12.661888
21.024944	745.212128	12.666893
21.211626	761.256912	12.671898
20.938930	749.234885	12.676903
20.630062	742.845386	12.681907
20.528242	743.609272	12.686912
21.211793	749.354235	12.691917
20.895468	745.656294	12.696922
20.582273	738.447445	12.701927
21.129620	744.029620	12.706931
20.910478	739.379441	12.711936
21.044497	730.720966	12.716941
20.578008	727.113215	12.721946
20.545328	728.845391	12.726951
20.900488	744.095284	12.731955
20.989344	760.838513	12.736960
21.246058	749.452739	12.741965
20.791830	744.478919	12.746970
20.747847	743.666038	12.751975
20.779605	730.130431	12.756979
20.276105	735.888094	12.761984
20.661388	747.294761	12.766989
21.043622	752.258279	12.771994
20.940035	763.075858	12.776999
21.029969	753.598050	12.782003
20.837720	758.604311	12.787008
21.162893	762.741121	12.792013
21.074512	760.353584	12.797018
20.864373	743.290936	12.802023
21.161289	741.067460	12.807027
20.842747	740.728893	12.812032
20.815460	735.518241	12.817037
20.913216	738.775078	12.822042
20.917948	739.143488	12.827047
20.776007	739.227777	12.832051
20.539601	736.149471	12.837056
20.881324	743.483375	12.842061
20.813162	767.012273	12.847066
21.080230	760.838423	12.852071
20.935685	746.427296	12.857075
20.847746	745.829590	12.862080
21.001101	737.377769	12.867085
20.788856	739.488681	12.872090
20.810519	733.874395	12.877095
20.926634	738.818850	12.882099
20.640346	740.015871	12.887104
21.148361	732.660275	12.892109
21.017098	737.464408	12.897114
21.008487	738.379013	12.902119
21.162819	732.136420	12.907123
21.075681	738.930001	12.912128
21.008344	737.849601	12.917133
20.814372	744.237588	12.922138
20.855367	733.919169	12.927143
20.842981	740.552590	12.932147
21.053132	738.248333	12.937152
21.348870	739.038699	12.942157
21.073843	744.070774	12.947162
21.047035	744.281784	12.952167
20.946220	744.752187	12.957171
20.779383	745.677836	12.962176
21.239141	740.137180	12.967181
20.818054	750.104921	12.972186
20.947903	737.928809	12.977191
21.057624	732.891854	12.982195
20.593186	726.178658	12.987200
20.891303	729.509195	12.992205
20.912812	732.732458	12.997210
20.810118	740.968325	13.002215
20.919426	729.180286	13.007219
20.919776	730.039843	13.012224
20.828275	713.940780	13.017229
20.623338	723.419851	13.022234
20.958425	737.121169	13.027239
21.253838	735.945064	13.032243
20.671582	728.255569	13.037248
20.976215	715.567459	13.042253
20.715346	721.276956	13.047258
20.583383	720.996942	13.052263
21.147150	736.122089	13.057267
20.958814	732.741217	13.062272
20.834449	719.719391	13.067277
20.681279	720.836830	13.072282
20.927796	727.359562	13.077287
21.004013	730.058420	13.082291
20.614886	737.090983	13.087296
20.820032	744.828307	13.092301
21.089469	752.274674	13.097306
20.995599	744.680745	13.102311
20.858188	725.610032	13.107315
20.630663	725.056669	13.112320
21.006894	742.802748	13.117325
20.602437	750.933781	13.122330
21.077575	745.445865	13.127335
21.014806	747.280617	13.132339
20.804289	740.626266	13.137344
20.883407	718.031118	13.142349
20.899534	726.949791	13.147354
20.869620	736.784166	13.152359
20.966128	727.179166	13.157363
20.868545	723.982524	13.162368
20.815561	720.826078	13.167373
20.422763	729.732702	13.172378
20.714928	738.392883	13.177383
21.106774	744.775745	13.182387
20.942940	757.132624	13.187392
21.207233	751.474901	13.192397
20.750247	733.469162	13.197402
21.079768	728.558005	13.202407
20.890721	720.107188	13.207411
20.724609	730.999373	13.212416
21.111779	717.421283	13.217421
20.972645	734.151958	13.222426
20.719783	728.959940	13.227431
20.929359	722.609189	13.232435
20.542933	734.154701	13.237440
20.924995	730.772742	13.242445
20.938422	722.884158	13.247450
20.584642	724.304838	13.252455
21.196945	734.735393	13.257459
20.899544	730.640187	13.262464
21.021405	725.650186	13.267469
20.833182	724.557528	13.272474
20.781791	727.592138	13.277479
21.227493	721.219497	13.282483
21.152852	723.830447	13.287488
21.104712	718.250955	13.292493
21.010612	731.905600	13.297498
20.874574	716.900192	13.302503
21.002811	718.231376	13.307507
20.711117	726.388566	13.312512
21.048146	727.312699	13.317517
21.021521	729.704673	13.322522
21.055385	725.272773	13.327527
21.271859	726.911592	13.332531
20.816209	733.927955	13.337536
21.133253	720.875150	13.342541
21.047025	722.601674	13.347546
20.593992	712.131824	13.352551
21.231667	716.081579	13.357555
20.737617	713.665709	13.362560
21.030017	699.841758	13.367565
20.418877	697.808853	13.372570
20.590455	717.065979	13.377575
21.198854	717.429572	13.382579
20.822135	731.477812	13.387584
21.031056	737.183350	13.392589
20.878793	738.155560	13.397594
21.231810	716.086028	13.402599
20.988924	704.383357	13.407603
20.395754	716.921434	13.412608
21.065662	705.225355	13.417613
20.830417	708.992628	13.422618
20.749552	709.969219	13.427623
21.183585	710.212385	13.432627
20.821012	706.515523	13.437632
20.801930	698.707045	13.442637
20.887302	704.746888	13.447642
20.777639	690.348388	13.452647
20.969177	695.345456	13.457651
20.634965	697.852718	13.462656
21.155329	703.748273	13.467661
20.588272	709.912679	13.472666
20.698392	698.123747	13.477671
20.825805	706.848822	13.482675
21.211569	721.216998	13.487680
21.144672	714.553945	13.492685
20.987359	713.342814	13.497690
20.913149	705.466641	13.502695
20.833746	701.769560	13.507699
20.714628	699.238697	13.512704
21.006714	701.873156	13.517709
21.118855	706.692863	13.522714
20.618468	701.583702	13.527719
21.019706	698.652867	13.532723
20.822539	704.964862	13.537728
21.073621	692.276639	13.542733
20.876022	698.013884	13.547738
20.754752	698.743022	13.552743
20.980149	704.072170	13.557747
20.539308	709.550951	13.562752
20.522504	697.063152	13.567757
20.736089	699.390000	13.572762
20.411979	711.177085	13.577767
21.013398	720.885523	13.582771
20.987419	722.298075	13.587776
21.154773	730.746339	13.592781
20.894904	717.730357	13.597786
20.938970	706.446344	13.602791
21.061866	696.199259	13.607795
20.511334	704.372489	13.612800
20.759830	701.748299	13.617805
20.849096	705.574990	13.622810
21.025208	721.652956	13.627815
21.273194	709.967397	13.632819
21.059220	707.322348	13.637824
20.940613	705.245579	13.642829
20.598709	708.343868	13.647834
20.690553	705.804588	13.652839
20.809089	705.852063	13.657843
20.581467	706.675437	13.662848
20.820570	704.760817	13.667853
20.898179	713.956690	13.672858
20.993580	718.322529	13.677863
20.979218	708.281049	13.682867
20.715370	709.900278	13.687872
21.039483	702.119064	13.692877
20.928752	707.778589	13.697882
20.876487	704.762385	13.702887
21.045715	704.223804	13.707891
20.485426	716.116374	13.712896
20.596459	718.924797	13.717901
20.950789	721.910465	13.722906
21.186144	729.363833	13.727911
20.942984	716.846674	13.732915
20.657257	713.506572	13.737920
20.993177	707.504695	13.742925
20.906962	706.753747	13.747930
20.914343	705.565235	13.752935
21.064695	701.664347	13.757939
20.912353	713.821442	13.762944
21.064818	706.718116	13.767949
21.045616	702.779614	13.772954
20.916421	705.682334	13.777959
20.923324	705.219318	13.782963
20.960388	704.542539	13.787968
21.562764	701.740477	13.792973
21.054086	710.421925	13.797978
20.880334	709.531970	13.802983
21.208531	712.774125	13.807987
20.868297	713.339485	13.812992
21.054815	708.731850	13.817997
20.843885	712.539401	13.823002
20.887319	707.129817	13.828007
20.880991	694.750739	13.833011
20.925998	701.709312	13.838016
21.121582	684.596215	13.843021
20.467294	686.470109	13.848026
20.706509	700.368038	13.853031
20.988240	702.709250	13.858035
20.796183	707.424506	13.863040
21.138093	703.412638	13.868045
20.986808	704.132371	13.873050
20.765344	690.708153	13.878055
20.630800	683.273713	13.883059
20.802924	698.016572	13.888064
21.190365	700.008176	13.893069
20.814680	690.361815	13.898074
20.808804	694.508828	13.903079
21.207824	686.333253	13.908083
20.594269	696.563474	13.913088
20.712503	693.379725	13.918093
20.907795	706.213095	13.923098
20.794765	703.062288	13.928103
20.877082	702.666094	13.933107
20.570389	710.192503	13.938112
21.257058	703.835842	13.943117
20.989377	706.344322	13.948122
20.602072	695.864789	13.953127
20.943618	687.485486	13.958131
20.845816	710.436319	13.963136
21.106702	697.645600	13.968141
20.854419	698.953893	13.973146
20.656011	687.476749	13.978151
20.784280	697.363141	13.983155
20.452923	715.214948	13.988160
21.092322	710.404188	13.993165
20.810397	717.284022	13.998170
20.671954	709.612063	14.003175
21.252658	713.826378	14.008179
20.776024	718.215644	14.013184
20.894490	714.680183	14.018189
21.003389	716.546708	14.023207
20.944851	712.216346	14.028224
20.984646	704.815579	14.033242
20.639963	710.991156	14.038259
20.727871	706.719232	14.043277
20.967870	716.023013	14.048295
20.518096	724.471008	14.053312
20.949138	721.442059	14.058330
20.719512	723.732909	14.063347
21.019290	723.394241	14.068365
20.945095	719.487932	14.073383
21.078347	720.085006	14.078400
20.889968	717.513492	14.083418
20.752066	721.844022	14.088435
21.241202	722.761849	14.093453
20.858730	723.655104	14.098471
20.948519	727.568659	14.103488
21.587283	722.497884	14.108506
20.691910	723.089139	14.113523
20.914328	732.054398	14.118541
20.861181	737.947540	14.123559
21.121531	748.299634	14.128576
21.767015	746.537333	14.133594
21.307994	756.729685	14.138611
21.391555	755.365312	14.143629
21.367898	757.042885	14.148647
21.388237	750.917741	14.153664
21.511678	751.667388	14.158682
21.162437	748.806929	14.163699
21.426832	751.803907	14.168717
21.608251	755.448031	14.173735
21.457188	755.193854	14.178752
21.262843	743.267191	14.183770
21.122821	763.073067	14.188787
21.380169	760.806396	14.193805
21.566321	759.730819	14.198823
21.504988	763.312993	14.203840
21.420655	758.826286	14.208858
21.509211	760.929543	14.213875
21.479781	765.222336	14.218893
21.425918	766.069474	14.223911
21.591175	761.093084	14.228928
22.011707	754.374015	14.233946
21.525789	761.174591	14.238963
21.615589	754.036377	14.243981
21.712978	761.149748	14.248999
21.580209	762.607204	14.254016
21.789951	755.220203	14.259034
21.582836	762.641684	14.264051
21.640188	762.974021	14.269069
21.717994	764.198123	14.274087
21.880042	762.857409	14.279104
21.760198	756.995288	14.284122
21.515793	768.188440	14.289139
21.759636	764.313188	14.294157
21.668773	758.682390	14.299175
21.255768	764.145315	14.304192
21.599694	769.264149	14.309210
21.673773	787.171924	14.314227
21.978032	783.724321	14.319245
21.931043	782.739408	14.324263
21.956036	790.410166	14.329280
22.082014	790.994246	14.334298
21.792209	801.079417	14.339315
22.359809	793.478022	14.344333
22.245570	790.158512	14.349351
22.268428	788.800672	14.354368
22.329464	797.041398	14.359386
22.158889	795.693960	14.364403
21.903887	781.250724	14.369421
21.999704	785.841290	14.374439
22.078243	795.765463	14.379456
22.245202	794.342169	14.384474
22.152521	800.051310	14.389491
21.809348	797.803339	14.394509
22.208794	798.507393	14.399527
22.033032	793.984922	14.404544
22.113749	801.833984	14.409562
22.382964	799.983829	14.414579
22.216982	800.262128	14.419597
21.975203	791.534582	14.424615
22.169777	797.319026	14.429632
22.172923	792.720831	14.434650
22.089777	801.149719	14.439667
22.114941	798.750193	14.444685
22.457677	811.806527	14.449703
22.270850	828.952170	14.454720
22.712808	815.523998	14.459738
22.433212	821.174873	14.464755
22.647975	827.028467	14.469773
22.778177	826.117534	14.474791
22.342059	810.188368	14.479808
22.567833	814.072392	14.484826
22.735755	827.133027	14.489843
22.656299	822.612490	14.494861
22.961397	815.444626	14.499879
22.469785	808.795511	14.504896
22.578028	804.369308	14.509914
22.765654	808.421433	14.514931
22.659998	804.358101	14.519949
22.823731	801.692660	14.524967
22.412916	807.510746	14.529984
22.634921	810.973809	14.535002
22.549883	821.042064	14.540019
22.815485	822.215770	14.545037
23.088939	822.527797	14.550055
23.060333	824.346164	14.555072
23.267728	827.876054	14.560090
22.851440	811.327111	14.565107
22.599664	800.578292	14.570125
22.977738	814.048980	14.575143
22.969762	825.075480	14.580160
23.216423	816.933817	14.585178
22.980119	804.812453	14.590195
22.959824	794.039302	14.595213
23.236405	794.519140	14.600231
23.116725	800.666732	14.605248
22.974282	789.802957	14.610266
22.963211	806.745940	14.615283
22.972738	807.192869	14.620301
22.614227	798.752918	14.625319
22.611469	821.492623	14.630336
23.089625	823.115335	14.635354
23.373055	824.254737	14.640371
23.201293	838.192234	14.645389
23.181654	823.970960	14.650407
23.119291	834.018304	14.655424
23.278282	827.502934	14.660442
23.192182	825.690572	14.665459
23.249762	824.453030	14.670477
23.220439	822.452291	14.675495
22.854934	830.739046	14.680512
23.137322	831.004032	14.685530
22.987410	821.646776	14.690547
23.015973	825.134405	14.695565
23.567084	848.655676	14.700583
23.575734	840.621173	14.705600
23.445358	831.094058	14.710618
23.230238	844.508379	14.715635
23.613446	852.655281	14.720653
23.745785	852.187590	14.725671
23.488086	847.958164	14.730688
23.411874	831.163052	14.735706
23.388262	841.356801	14.740723
23.459838	855.699088	14.745741
23.753949	852.920036	14.750759
23.439678	862.055918	14.755776
23.552391	859.442648	14.760794
23.562942	860.790740	14.765811
23.587255	856.003536	14.770829
23.852496	857.726276	14.775847
23.880196	855.164318	14.780864
23.933968	853.565592	14.785882
23.856627	859.327365	14.790899
23.597467	851.179844	14.795917
24.117082	848.850881	14.800935
23.991893	855.987215	14.805952
23.759892	861.869609	14.810970
23.822696	855.169797	14.815987
24.042140	853.933177	14.821005
24.327347	849.931758	14.826023
24.114953	846.951927	14.831040
24.142888	830.544464	14.836058
24.080525	819.744970	14.841075
23.874271	820.951464	14.846093
24.006515	808.365484	14.851111
23.680465	819.406533	14.856128
23.821318	835.468039	14.861146
24.134187	849.639703	14.866163
24.128674	852.028532	14.871181
24.533984	842.633043	14.876199
24.056395	847.837318	14.881216
24.080278	846.153699	14.886234
24.272824	845.206081	14.891251
24.307272	852.040105	14.896269
24.339725	844.730099	14.901287
24.051833	831.062825	14.906304
24.341917	836.838344	14.911322
23.932421	846.782191	14.916339
24.242005	845.084465	14.921357
24.536312	835.878141	14.926375
23.871264	845.526127	14.931392
23.981734	843.858586	14.936410
24.294430	844.804563	14.941427
24.402177	841.131891	14.946445
24.526079	844.863862	14.951463
24.219662	845.776453	14.956480
24.036538	843.820692	14.961498
24.054384	846.378823	14.966515
24.533508	856.352402	14.971533
24.831433	857.605897	14.976551
24.553744	854.230647	14.981568
24.627899	848.726075	14.986586
24.541960	846.669871	14.991603
24.227912	853.013650	14.996621
24.538017	865.241551	15.001639
24.848482	872.022123	15.006656
24.778627	871.346013	15.011674
25.000182	874.271199	15.016691
24.609750	873.720150	15.021709
25.067706	864.267488	15.026727
24.975069	860.095100	15.031744
24.720490	851.133610	15.036762
24.980235	853.829337	15.041779
24.749152	848.508727	15.046797
24.718392	837.649125	15.051815
24.559624	855.196155	15.056832
25.043969	858.486829	15.061850
25.152861	867.795890	15.066867
24.966067	864.041205	15.071885
25.277098	860.153639	15.076903
25.078134	851.538776	15.081920
24.902096	843.749228	15.086938
25.142581	846.196346	15.091955
24.649939	842.322137	15.096973
25.189536	861.226963	15.101991
25.068544	871.812211	15.107008
25.353358	869.635523	15.112026
25.137667	864.290430	15.117043
24.922917	875.916227	15.122061
25.298881	876.650772	15.127079
25.106248	879.289670	15.132096
25.060549	892.290056	15.137114
25.332586	877.589634	15.142131
25.387053	884.749237	15.147149
25.638593	876.578448	15.152167
25.142308	881.900544	15.157184
25.426053	881.342639	15.162202
25.322724	873.750686	15.167219
25.175294	880.248797	15.172237
25.376003	864.483835	15.177255
25.398357	870.022076	15.182272
25.337574	877.673528	15.187290
25.735464	870.940714	15.192307
25.290723	875.419327	15.197325
25.535885	874.460169	15.202343
25.547831	871.243208	15.207360
25.355351	883.460051	15.212378
25.462538	870.827678	15.217395
25.141590	882.717379	15.222413
25.539869	872.942327	15.227431
25.486083	877.349147	15.232448
25.406902	874.862433	15.237466
25.399050	877.116362	15.242483
25.553714	886.970256	15.247501
25.863558	895.921673	15.252519
25.872204	898.931159	15.257536
25.442138	902.020055	15.262554
25.898001	893.288141	15.267571
25.665666	911.935487	15.272589
26.063523	911.386121	15.277607
26.106689	916.048046	15.282624
26.060185	906.968393	15.287642
26.095308	891.934515	15.292659
25.852152	892.640395	15.297677
25.625039	886.207029	15.302695
25.769070	901.135543	15.307712
26.131443	907.752126	15.312730
26.260194	904.140581	15.317747
25.869453	915.089776	15.322765
26.141485	901.624135	15.327783
26.038971	912.417247	15.332800
26.163359	910.511528	15.337818
26.311817	906.470557	15.342835
26.356610	908.667331	15.347853
26.253070	901.394717	15.352871
26.226388	906.427995	15.357888
25.991979	906.143064	15.362906
26.350986	906.823688	15.367923
26.003762	914.376129	15.372941
26.317675	903.673859	15.377959
26.644875	910.856040	15.382976
26.489777	905.671152	15.387994
26.477088	907.897543	15.393011
26.411157	912.311030	15.398029
26.583294	905.504096	15.403047
26.584145	910.512535	15.408064
26.384550	907.755589	15.413082
26.627920	902.157943	15.418099
26.504506	910.280290	15.423117
26.712810	906.309997	15.428135
26.548070	908.376598	15.433152
26.344806	906.273032	15.438170
26.394009	912.824737	15.443187
26.642100	909.883131	15.448205
26.652223	909.428640	15.453223
26.431965	917.132289	15.458240
26.344124	921.634215	15.463258
26.933545	906.751011	15.468275
26.797259	915.982805	15.473293
26.734392	908.396965	15.478311
26.723268	914.382575	15.483328
26.826808	904.824395	15.488346
26.847780	903.872679	15.493363
26.449956	904.703899	15.498381
26.647516	904.749614	15.503399
26.613670	916.958486	15.508416
26.493044	919.629950	15.513434
27.217765	911.894897	15.518451
27.229218	932.724462	15.523469
27.108544	914.621316	15.528487
27.028532	908.486943	15.533504
26.707516	911.890351	15.538522
27.062886	913.178733	15.543539
27.125745	930.923310	15.548557
27.334349	935.083808	15.553575
27.683687	935.704628	15.558592
27.206681	920.387466	15.563610
27.212373	908.252586	15.568627
27.249972	898.050560	15.573645
27.070397	896.841399	15.578663
27.166110	895.464064	15.583680
27.354799	919.988628	15.588698
27.355511	914.171708	15.593715
27.384736	926.468055	15.598733
27.513482	921.640578	15.603751
27.372414	901.327490	15.608768
27.016531	909.733874	15.613786
27.597024	923.096876	15.618803
27.325887	933.084780	15.623821
27.156015	929.437489	15.628839
27.589871	929.533604	15.633856
27.424606	929.940776	15.638874
27.409677	924.524315	15.643891
27.470888	927.597781	15.648909
27.570914	928.270949	15.653927
27.698237	926.824076	15.658944
27.499299	926.747415	15.663962
27.451965	927.510152	15.668979
27.189596	929.117281	15.673997
27.602107	930.898338	15.679015
27.573989	931.975757	15.684032
27.800089	943.962297	15.689050
28.048944	947.226059	15.694067
27.844206	947.353241	15.699085
27.932190	936.839562	15.704103
28.016831	927.713811	15.709120
27.511756	932.850141	15.714138
28.034327	940.781386	15.719155
28.130314	957.383431	15.724173
28.076817	947.861280	15.729191
27.899161	926.575584	15.734208
27.788243	925.574117	15.739226
28.046245	944.409136	15.744243
28.212591	950.056574	15.749261
28.001114	951.809743	15.754279
28.439165	961.495795	15.759296
27.813673	957.781168	15.764314
28.208398	947.270468	15.769331
28.142136	960.769691	15.774349
28.049283	964.279864	15.779367
28.504488	950.427891	15.784384
28.292600	952.802462	15.789402
28.404652	951.196003	15.794419
28.506672	957.430996	15.799437
28.635589	952.345509	15.804455
28.809861	943.534210	15.809472
28.658713	932.360262	15.814490
29.063593	915.052600	15.819507
29.203746	908.884685	15.824525
28.506377	917.191384	15.829543
28.840223	917.989278	15.834560
28.637296	909.239734	15.839578
28.657750	910.299966	15.844595
28.615365	915.824955	15.849613
28.674640	914.475452	15.854631
28.605029	913.426499	15.859648
28.280550	920.844757	15.864666
28.356937	910.735635	15.869683
28.624507	913.848543	15.874701
28.383986	914.234684	15.879719
28.602206	914.863832	15.884736
28.559315	908.893422	15.889754
28.617433	910.523364	15.894771
28.658712	914.366057	15.899789
28.548386	912.466313	15.904807
29.037986	921.307282	15.909824
29.103316	932.856993	15.914842
29.181811	919.554336	15.919859
28.845628	911.593668	15.924877
28.759128	923.870718	15.929895
29.281123	929.002108	15.934912
28.921668	939.134662	15.939930
28.874752	931.904910	15.944947
28.953994	949.352745	15.949965
29.013066	945.859268	15.954983
29.243460	946.439286	15.960000
29.084042	952.700244	15.965018
29.357950	942.532856	15.970035
29.341024	942.593903	15.975053
29.158285	948.627348	15.980071
29.411248	945.670801	15.985088
29.275541	947.890078	15.990106
29.383851	934.785568	15.995123
29.485943	940.913579	16.000141
29.240207	940.614723	16.005159
29.539168	931.730062	16.010176
29.369869	943.152039	16.015194
29.252228	937.619823	16.020211
29.763164	938.663175	16.025229
29.574324	941.675853	16.030247
29.575625	936.193879	16.035264
29.656149	944.343493	16.040282
29.666514	931.259327	16.045299
29.895699	941.030588	16.050317
29.232829	943.659554	16.055335
29.571191	931.487326	16.060352
29.381678	936.747930	16.065370
29.407621	936.849330	16.070387
29.523284	928.546030	16.075405
29.691390	942.567845	16.080423
29.801447	940.307337	16.085440
29.698324	944.660699	16.090458
29.802667	930.210336	16.095475
29.764168	942.110092	16.100493
29.549408	940.249023	16.105511
29.985624	935.554970	16.110528
29.648076	944.375296	16.115546
30.173111	955.942940	16.120563
30.209369	951.452669	16.125581
30.319115	947.210225	16.130599
30.246661	940.657787	16.135616
30.038215	937.814158	16.140634
29.870307	931.185715	16.145651
29.978174	940.826889	16.150669
29.846206	954.547369	16.155687
30.316773	959.123837	16.160704
30.287485	960.745704	16.165722
30.302032	971.982653	16.170739
30.635923	962.909934	16.175757
30.546598	954.939757	16.180775
30.384329	936.088175	16.185792
29.708134	950.318589	16.190810
29.934343	958.468569	16.195827
30.122120	970.890675	16.200845
30.207117	972.263083	16.205863
30.440607	969.381996	16.210880
30.703198	969.008357	16.215898
30.270463	967.534404	16.220915
30.427916	970.719942	16.225933
30.202909	967.215140	16.230951
30.647362	957.401208	16.235968
30.365405	970.283619	16.240986
30.681353	965.097511	16.246003
30.602342	975.838159	16.251021
30.386827	994.739328	16.256039
30.904677	992.671745	16.261056
30.759459	995.809609	16.266074
30.791188	999.408458	16.271091
30.905833	1000.008513	16.276109
30.709669	992.042771	16.281127
30.979181	986.088570	16.286144
30.846215	998.868592	16.291162
30.936136	991.554065	16.296179
31.154288	991.066392	16.301197
30.717710	992.960859	16.306215
31.237423	983.166366	16.311232
31.251687	986.248905	16.316250
31.134077	990.477178	16.321267
31.590132	982.709435	16.326285
31.116214	978.635577	16.331303
31.066074	959.119575	16.336320
30.976001	971.903744	16.341338
31.336044	986.977218	16.346355
31.623482	991.881776	16.351373
31.027071	984.549304	16.356391
31.410568	976.349548	16.361408
31.299607	987.672594	16.366426
31.325315	993.035743	16.371443
31.485604	991.924949	16.376461
31.563771	985.252514	16.381479
31.596416	976.427605	16.386496
31.303555	970.265806	16.391514
31.574453	979.382362	16.396531
31.690066	984.647800	16.401549
31.376200	982.105690	16.406567
31.648385	977.009928	16.411584
31.470219	992.051272	16.416602
31.411914	993.492155	16.421619
31.427039	992.816642	16.426637
31.498791	999.542540	16.431655
31.945272	991.568682	16.436672
31.761278	990.913916	16.441690
31.413065	991.359706	16.446707
31.731404	989.912249	16.451725
31.416756	1003.271805	16.456743
31.530958	997.185069	16.461760
31.648218	993.822298	16.466778
31.710642	1004.872313	16.471795
31.876406	1012.635567	16.476813
31.936419	1018.754591	16.481831
32.264478	1011.166122	16.486848
32.096018	1015.179145	16.491866
31.748290	1018.567961	16.496883
32.003020	1006.810127	16.501901
32.061766	1016.073799	16.506919
32.406144	1015.644643	16.511936
32.143377	1010.483181	16.516954
32.406027	1011.251538	16.521971
32.528582	1007.225682	16.526989
32.335470	1009.348731	16.532007
32.514284	1003.471909	16.537024
32.569987	1003.857997	16.542042
32.274276	994.652869	16.547059
32.174941	993.264163	16.552077
32.292779	1007.423045	16.557095
32.640781	997.824241	16.562112
32.366679	993.894686	16.567130
32.120459	1002.904971	16.572147
32.574891	1009.865566	16.577165
32.492754	1014.302117	16.582183
32.603799	1014.227925	16.587200
32.278561	1009.291929	16.592218
32.044276	1011.254807	16.597235
32.456968	1006.652572	16.602253
32.136735	1012.528649	16.607271
32.108056	1012.001693	16.612288
32.537358	1033.738453	16.617306
32.784776	1040.417476	16.622323
33.011759	1024.102316	16.627341
32.874622	1040.744784	16.632359
33.347768	1029.166026	16.637376
32.871007	1029.390076	16.642394
33.043388	1034.487603	16.647411
33.203433	1030.071946	16.652429
33.135869	1041.860016	16.657447
33.385653	1029.014427	16.662464
33.299465	1008.931532	16.667482
33.342900	1009.509911	16.672499
32.939282	1004.375635	16.677517
32.875959	1002.380294	16.682535
33.082945	995.515851	16.687552
33.222098	1017.847844	16.692570
33.076433	1031.469908	16.697587
33.241725	1028.914289	16.702605
33.221116	1033.328449	16.707623
33.228474	1035.837950	16.712640
33.260574	1027.838929	16.717658
33.467780	1029.224884	16.722675
33.430623	1030.506670	16.727693
33.503413	1030.756328	16.732711
33.391237	1027.974404	16.737728
33.453042	1028.925804	16.742746
33.343238	1036.039322	16.747763
33.563956	1034.122943	16.752781
33.299952	1027.154281	16.757799
32.971068	1027.740133	16.762816
33.355161	1035.814640	16.767834
33.565756	1049.235183	16.772851
34.058250	1057.397805	16.777869
33.921528	1061.147804	16.782887
33.760279	1037.064080	16.787904
33.925577	1023.464340	16.792922
33.468503	1033.098153	16.797939
33.723218	1045.893463	16.802957
33.743873	1055.234021	16.807975
33.838419	1058.085122	16.812992
34.031631	1052.470250	16.818010
33.649395	1057.857588	16.823027
33.934939	1050.922388	16.828045
33.984492	1060.626426	16.833063
33.964988	1063.366731	16.838080
34.046258	1061.806068	16.843098
34.292207	1062.130355	16.848115
34.305305	1058.395647	16.853133
34.459416	1054.388340	16.858151
34.366860	1053.763032	16.863168
34.219713	1051.233645	16.868186
34.116357	1057.160092	16.873203
34.428999	1052.090885	16.878221
34.216708	1053.836330	16.883239
34.486067	1046.898995	16.888256
34.394436	1046.097361	16.893274
34.122950	1048.009548	16.898291
34.638445	1045.852673	16.903309
34.423499	1046.714507	16.908327
34.168962	1048.699495	16.913344
34.410126	1056.274569	16.918362
34.653510	1072.750992	16.923379
34.867138	1069.316205	16.928397
34.598195	1067.374100	16.933415
34.833702	1071.258215	16.938432
34.761218	1053.710348	16.943450
34.418551	1077.627800	16.948467
35.166323	1071.820655	16.953485
35.124755	1085.915375	16.958503
35.122617	1068.474248	16.963520
35.234421	1048.856792	16.968538
35.050116	1048.667685	16.973555
35.098040	1038.765932	16.978573
34.993802	1046.029577	16.983591
34.891324	1048.172783	16.988608
35.158631	1040.667920	16.993626
34.728523	1051.134287	16.998643
35.090348	1042.675258	17.003661
35.110616	1047.697951	17.008679
35.328325	1062.608590	17.013696
35.334762	1050.569426	17.018714
35.068456	1060.572377	17.023731
35.119333	1059.688239	17.028749
35.232801	1070.660952	17.033767
35.026256	1077.187454	17.038784
35.471469	1076.056380	17.043802
35.184939	1081.137455	17.048819
35.231024	1075.250312	17.053837
35.361859	1084.436464	17.058855
35.270257	1075.006823	17.063872
35.068950	1076.048953	17.068890
35.043988	1083.380197	17.073907
35.378427	1089.436607	17.078925
35.524923	1108.006480	17.083943
35.530137	1107.631416	17.088960
35.821013	1101.208147	17.093978
35.786616	1105.663854	17.098995
35.852127	1105.908382	17.104013
35.999800	1105.526327	17.109031
35.959522	1110.308588	17.114048
36.227976	1094.935266	17.119066
35.807474	1094.521135	17.124083
35.849425	1093.671453	17.129101
35.744166	1100.027656	17.134119
36.028149	1099.142517	17.139136
35.976599	1108.740016	17.144154
35.757369	1103.826406	17.149171
35.934679	1100.235383	17.154189
36.157628	1105.982394	17.159207
36.081844	1105.697326	17.164224
36.164891	1108.803528	17.169242
36.160525	1110.680985	17.174259
36.363535	1101.262540	17.179277
36.183685	1113.941603	17.184295
36.166810	1106.566973	17.189312
36.318585	1097.516925	17.194330
35.884626	1106.453397	17.199347
36.007234	1107.258252	17.204365
36.461995	1116.192987	17.209383
36.668268	1131.265969	17.214400
36.866898	1128.484792	17.219418
36.470902	1125.276209	17.224435
36.747889	1111.693181	17.229453
36.625691	1116.732327	17.234471
36.570197	1109.005207	17.239488
36.628441	1119.033513	17.244506
36.469535	1139.222011	17.249523
36.283652	1137.741702	17.254541
36.511106	1136.662657	17.259559
36.515811	1134.607685	17.264576
37.067683	1134.987001	17.269594
36.935521	1137.954500	17.274611
36.894668	1136.249712	17.279629
36.867064	1132.865969	17.284647
36.916233	1133.344338	17.289664
36.908685	1137.589706	17.294682
36.892240	1139.373139	17.299699
37.337587	1135.596213	17.304717
37.017393	1130.358923	17.309735
36.886150	1129.481806	17.314752
37.221942	1135.948578	17.319770
37.088305	1150.960962	17.324787
37.417598	1148.879387	17.329805
37.102178	1154.805090	17.334823
37.332454	1162.941954	17.339840
37.770236	1160.819479	17.344858
37.628413	1156.349683	17.349875
37.580412	1140.946559	17.354893
37.535327	1126.032197	17.359911
37.310771	1125.505016	17.364928
37.265401	1126.964298	17.369946
37.303812	1140.063177	17.374963
37.544042	1151.515955	17.379981
37.460308	1144.878707	17.384999
37.439980	1163.582224	17.390016
37.599311	1155.350481	17.395034
37.445143	1162.225745	17.400051
37.465035	1164.140239	17.405069
37.513619	1156.920311	17.410087
37.370902	1158.709728	17.415104
37.844928	1170.348602	17.420122
37.896335	1184.604769	17.425139
37.938094	1185.273085	17.430157
38.290616	1188.470033	17.435175
37.776074	1184.591356	17.440192
38.507412	1188.997321	17.445210
38.522271	1167.877194	17.450227
38.313397	1155.850260	17.455245
38.421552	1155.255857	17.460263
38.066290	1155.318956	17.465280
38.332028	1146.521262	17.470298
38.123257	1153.960508	17.475315
37.925558	1149.531086	17.480333
38.363489	1156.994606	17.485351
38.257460	1174.325970	17.490368
38.396047	1180.357026	17.495386
38.335761	1186.020253	17.500403
38.425649	1184.895505	17.505421
38.413396	1195.043646	17.510439
38.357554	1190.294284	17.515456
38.372924	1175.758767	17.520474
38.532428	1185.662430	17.525491
38.483301	1180.550204	17.530509
38.473141	1182.622076	17.535527
38.417243	1187.768651	17.540544
38.728614	1178.507481	17.545562
38.353380	1184.302736	17.550579
38.744593	1201.235502	17.555597
39.104128	1210.978291	17.560615
39.140023	1215.627315	17.565632
39.220712	1205.139774	17.570650
38.986968	1197.680136	17.575667
38.739202	1193.071495	17.580685
38.738319	1198.256490	17.585703
38.640035	1203.851852	17.590720
39.267632	1204.791677	17.595738
39.081494	1204.917466	17.600755
39.124258	1216.326283	17.605773
39.321934	1218.676474	17.610791
39.262814	1218.893690	17.615808
39.403299	1209.785597	17.620826
39.346475	1212.656152	17.625843
39.288328	1212.624673	17.630861
39.702214	1214.831841	17.635879
39.545883	1213.944562	17.640896
39.650798	1207.222142	17.645914
39.613289	1212.713432	17.650931
39.345523	1213.877857	17.655949
39.290193	1213.257615	17.660967
39.215809	1207.169409	17.665984
39.475411	1208.897812	17.671002
39.429819	1213.144551	17.676019
39.389499	1215.537418	17.681037
39.606430	1203.429949	17.686055
39.285059	1224.495486	17.691072
39.636360	1230.774211	17.696090
39.648403	1234.769516	17.701107
39.711007	1233.288891	17.706125
40.005153	1230.508192	17.711143
39.995816	1244.822870	17.716160
40.185405	1227.542883	17.721178
40.059624	1236.781070	17.726195
39.954941	1238.580161	17.731213
40.200001	1235.363694	17.736231
40.143665	1235.040915	17.741248
40.390061	1240.837723	17.746266
40.084206	1238.391817	17.751283
40.230342	1230.533373	17.756301
40.558564	1233.765667	17.761319
40.465782	1229.797689	17.766336
40.572474	1224.062843	17.771354
40.544602	1230.895974	17.776371
40.642628	1232.159363	17.781389
40.711804	1220.721962	17.786407
40.473895	1234.286568	17.791424
40.448487	1225.121553	17.796442
40.483326	1230.143559	17.801459
40.559725	1234.742084	17.806477
40.390578	1234.876174	17.811495
40.179223	1236.413850	17.816512
40.697428	1243.677422	17.821530
40.897878	1256.544494	17.826547
40.920716	1263.806857	17.831565
41.199048	1264.143288	17.836583
41.052625	1259.277788	17.841600
40.618729	1244.794978	17.846618
40.819529	1257.131882	17.851635
40.766783	1263.633939	17.856653
41.318724	1265.161567	17.861671
40.803035	1269.135656	17.866688
41.038688	1258.099540	17.871706
41.215335	1264.108831	17.876723
41.027971	1264.860884	17.881741
41.074464	1254.679212	17.886759
40.993167	1262.741555	17.891776
41.182768	1256.482236	17.896794
41.104994	1267.790767	17.901811
41.020558	1264.666170	17.906829
41.409922	1278.281786	17.911847
41.129372	1297.583834	17.916864
41.274787	1287.140968	17.921882
41.816946	1293.681866	17.926899
41.576952	1301.818305	17.931917
41.775801	1290.132077	17.936935
41.974220	1295.041499	17.941952
41.813694	1287.016427	17.946970
41.786284	1295.600307	17.951987
41.910845	1291.001467	17.957005
42.130489	1289.506801	17.962023
41.792853	1293.509129	17.967040
42.075198	1285.314323	17.972058
42.283999	1280.626545	17.977075
41.529495	1284.645018	17.982093
41.909670	1277.844057	17.987111
41.811512	1297.963312	17.992128
41.906265	1291.923600	17.997146
41.719917	1287.456145	18.002163
41.959739	1290.954237	18.007181
41.898962	1287.547434	18.012199
41.768334	1286.958075	18.017216
42.160945	1296.882839	18.022234
42.679973	1304.136872	18.027251
42.271844	1305.792456	18.032269
42.510291	1304.017935	18.037287
42.681240	1317.437185	18.042304
42.707199	1305.253123	18.047322
42.314255	1290.033844	18.052339
42.365312	1298.691730	18.057357
42.447585	1307.882622	18.062375
42.486385	1317.942482	18.067392
42.691330	1309.286521	18.072410
42.797187	1304.819649	18.077427
42.786726	1309.800143	18.082445
42.792452	1311.103428	18.087463
42.558150	1317.969523	18.092480
42.987298	1308.105888	18.097498
43.187233	1315.626326	18.102515
42.871130	1317.658921	18.107533
43.053487	1297.850551	18.112551
42.696852	1312.239562	18.117568
42.695674	1301.927032	18.122586
43.075564	1306.601447	18.127603
42.643376	1311.595718	18.132621
42.972526	1329.375392	18.137639
43.286705	1344.083743	18.142656
43.268979	1340.448261	18.147674
43.075860	1338.877848	18.152691
42.821805	1338.880760	18.157709
43.216622	1335.656117	18.162727
43.122564	1350.788238	18.167744
42.867624	1348.452171	18.172762
43.264120	1352.494733	18.177779
43.365341	1364.864914	18.182797
43.907109	1372.011534	18.187815
43.913366	1367.604573	18.192832
43.772009	1366.098261	18.197850
43.996713	1369.205522	18.202867
43.922013	1358.686024	18.207885
43.947419	1341.208715	18.212903
43.807092	1346.725892	18.217920
43.352582	1343.839627	18.222938
44.075844	1360.527711	18.227955
44.269685	1371.152774	18.232973
44.203117	1363.027729	18.237991
44.307268	1356.242441	18.243008
43.960805	1338.044212	18.248026
44.337882	1342.080431	18.253043
44.143170	1344.147153	18.258061
44.316277	1334.678272	18.263079
44.614685	1331.588557	18.268096
44.229735	1331.228522	18.273114
44.284631	1329.165517	18.278131
43.997893	1338.212359	18.283149
44.598572	1341.954937	18.288167
44.545005	1353.377653	18.293184
44.354172	1369.190626	18.298202
44.552766	1366.481770	18.303219
44.364352	1363.913291	18.308237
44.661128	1368.201427	18.313255
44.558220	1373.438936	18.318272
44.615918	1359.771100	18.323290
44.970851	1360.568805	18.328307
44.701816	1368.544742	18.333325
44.703165	1360.536284	18.338343
44.430651	1370.106275	18.343360
44.644856	1363.367925	18.348378
44.986657	1360.760502	18.353395
44.748753	1368.173042	18.358413
44.754313	1368.502643	18.363431
44.937619	1386.505424	18.368448
44.699462	1402.887561	18.373466
44.924494	1392.010344	18.378483
44.939338	1396.667502	18.383501
45.164442	1389.361103	18.388519
44.641933	1391.381010	18.393536
44.787276	1398.222773	18.398554
45.135783	1417.342855	18.403571
45.275190	1425.821554	18.408589
45.664810	1418.218338	18.413607
45.586113	1413.752552	18.418624
45.524467	1412.886339	18.423642
45.844589	1411.240354	18.428659
45.697540	1406.090182	18.433677
45.882868	1401.409254	18.438695
45.836031	1405.086803	18.443712
45.722096	1414.765241	18.448730
46.071797	1408.777630	18.453747
46.228361	1415.790649	18.458765
46.211486	1409.639701	18.463783
46.314095	1395.381066	18.468800
45.934317	1392.083317	18.473818
46.072584	1388.800477	18.478835
45.768487	1388.575412	18.483853
45.765066	1381.660974	18.488871
45.867382	1392.376155	18.493888
46.027485	1405.064175	18.498906
46.360408	1401.196572	18.503923
46.190659	1410.814695	18.508941
46.347260	1396.923407	18.513959
46.420911	1408.143402	18.518976
46.318752	1408.564116	18.523994
46.465525	1404.656987	18.529011
46.384036	1409.327940	18.534029
46.152072	1404.057601	18.539047
46.195291	1411.102852	18.544064
45.962244	1408.700361	18.549082
46.232168	1419.338493	18.554099
46.233366	1445.899495	18.559117
46.253346	1436.643736	18.564135
46.608222	1448.572405	18.569152
46.478435	1449.154833	18.574170
46.502693	1437.096776	18.579187
46.733846	1452.516915	18.584205
47.142237	1463.084232	18.589223
47.357037	1466.488828	18.594240
47.144991	1461.699794	18.599258
47.464058	1454.299725	18.604275
47.219146	1458.833159	18.609293
47.126209	1440.374140	18.614311
47.408323	1432.547384	18.619328
47.338170	1445.795990	18.624346
47.430745	1440.609161	18.629363
46.871042	1440.099238	18.634381
47.167949	1446.651006	18.639399
47.335722	1462.439922	18.644416
47.342944	1461.476204	18.649434
47.739812	1452.710897	18.654451
47.597637	1461.023737	18.659469
47.782494	1461.964978	18.664487
48.025828	1457.705800	18.669504
47.853253	1464.245934	18.674522
48.075521	1457.562885	18.679539
47.681778	1454.567803	18.684557
47.336934	1452.299541	18.689575
47.799020	1448.969762	18.694592
47.447186	1449.932103	18.699610
47.808597	1447.058837	18.704627
47.829441	1454.891060	18.709645
47.869392	1468.114260	18.714663
48.367300	1484.100664	18.719680
48.251403	1489.389051	18.724698
48.505530	1481.042904	18.729715
48.423223	1467.326507	18.734733
48.217888	1453.593565	18.739751
48.062117	1451.842572	18.744768
48.234893	1468.635881	18.749786
48.367740	1473.568406	18.754803
48.406054	1484.366224	18.759821
48.333032	1487.244134	18.764839
48.752265	1483.844102	18.769856
48.484584	1489.757606	18.774874
48.512186	1472.633728	18.779891
48.524784	1486.828740	18.784909
48.396203	1480.673555	18.789927
48.666107	1481.538312	18.794944
48.409691	1487.555413	18.799962
48.496799	1482.067414	18.804979
48.601529	1498.939251	18.809997
48.860463	1501.707593	18.815015
49.052795	1504.818473	18.820032
48.824705	1507.162681	18.825050
48.989743	1502.568330	18.830067
49.015650	1506.410485	18.835085
49.173764	1508.627031	18.840103
49.433974	1503.331646	18.845120
49.118730	1504.041183	18.850138
49.608343	1506.845096	18.855155
49.257951	1506.842922	18.860173
49.123007	1510.328477	18.865191
49.541877	1506.255226	18.870208
49.399983	1506.779810	18.875226
49.630501	1503.545154	18.880243
49.482694	1522.840487	18.885261
49.673564	1528.166482	18.890279
49.758404	1539.608170	18.895296
49.601600	1544.325785	18.900314
50.014663	1531.883162	18.905331
49.785519	1541.954448	18.910349
49.977976	1539.971724	18.915367
50.186811	1524.212619	18.920384
50.027115	1540.670488	18.925402
50.103619	1536.532278	18.930419
49.911232	1535.065548	18.935437
50.092898	1529.807849	18.940455
50.042788	1537.217266	18.945472
49.753019	1544.704235	18.950490
50.053828	1531.862652	18.955507
50.067540	1535.783841	18.960525
50.031204	1541.946768	18.965543
50.302881	1546.262557	18.970560
50.510896	1557.503711	18.975578
50.748827	1558.985497	18.980595
50.705619	1563.294880	18.985613
50.855976	1560.096592	18.990631
50.900150	1553.432465	18.995648
50.665937	1539.293476	19.000666
50.841238	1531.417634	19.005683
50.740471	1532.176339	19.010701
50.833398	1531.365694	19.015719
50.759523	1539.213069	19.020736
51.243662	1550.320515	19.025754
51.319971	1546.479644	19.030771
51.144611	1541.288319	19.035789
51.236904	1537.759514	19.040807
51.078754	1526.115876	19.045824
50.845304	1527.990595	19.050842
51.067417	1535.041983	19.055859
51.206381	1552.787768	19.060877
51.063264	1551.481496	19.065895
51.619747	1557.232125	19.070912
51.599513	1561.073788	19.075930
51.345268	1556.433028	19.080947
51.693930	1555.721599	19.085965
51.311047	1553.426352	19.090983
51.779071	1552.157897	19.096000
51.491567	1556.208930	19.101018
51.766637	1554.161117	19.106035
51.720732	1549.065550	19.111053
51.464599	1549.738920	19.116071
51.591867	1552.089384	19.121088
51.437107	1553.706158	19.126106
51.848794	1548.263899	19.131123
51.893462	1573.967172	19.136141
51.828584	1584.125551	19.141159
52.056356	1583.832961	19.146176
52.021660	1588.736402	19.151194
52.241066	1579.042107	19.156211
52.518678	1578.050990	19.161229
52.340039	1580.278781	19.166247
52.554824	1581.265597	19.171264
52.239092	1576.570141	19.176282
52.117783	1580.242306	19.181299
52.245877	1585.023040	19.186317
52.094983	1578.327089	19.191335
52.399272	1577.391494	19.196352
52.380999	1585.621721	19.201370
52.605667	1592.486320	19.206387
52.704854	1605.496485	19.211405
52.647799	1605.028303	19.216423
53.291680	1599.792821	19.221440
53.119033	1601.524141	19.226458
53.026268	1603.648574	19.231475
53.300361	1600.633471	19.236493
53.091885	1601.459695	19.241511
53.358218	1590.578104	19.246528
53.234485	1597.921427	19.251546
53.080361	1586.305413	19.256563
53.618828	1587.476568	19.261581
53.161293	1576.856727	19.266599
53.244286	1576.381155	19.271616
53.054025	1583.951378	19.276634
53.064602	1587.716560	19.281651
53.493923	1592.358803	19.286669
53.139099	1595.376849	19.291687
53.426601	1584.310196	19.296704
53.498641	1595.525874	19.301722
53.581152	1594.554073	19.306739
53.541336	1593.723695	19.311757
53.029939	1602.161569	19.316775
53.529755	1604.245767	19.321792
53.651953	1621.641941	19.326810
53.757708	1625.928372	19.331827
54.089018	1619.626635	19.336845
53.572521	1624.749291	19.341863
54.037177	1613.878526	19.346880
53.802719	1622.179432	19.351898
53.857424	1632.675075	19.356915
54.418009	1642.040802	19.361933
54.242331	1643.457209	19.366951
54.574908	1651.182404	19.371968
54.442336	1655.971698	19.376986
54.771569	1647.913936	19.382003
54.810275	1639.723182	19.387021
54.528404	1637.682381	19.392039
54.897836	1612.872035	19.397056
54.819554	1615.128659	19.402074
54.558647	1613.212723	19.407091
54.770694	1613.448048	19.412109
54.439963	1629.016978	19.417127
54.857467	1634.399679	19.422144
54.830430	1637.509394	19.427162
54.770252	1639.319526	19.432179
55.295168	1642.633020	19.437197
54.902880	1645.986610	19.442215
55.159977	1634.385203	19.447232
54.796859	1640.151174	19.452250
54.595688	1649.529064	19.457267
54.858087	1645.839393	19.462285
55.510742	1660.442174	19.467303
55.366009	1662.803787	19.472320
55.362267	1677.228114	19.477338
55.395817	1657.224330	19.482355
55.758030	1661.753812	19.487373
55.582181	1672.013323	19.492391
55.989371	1663.590750	19.497408
56.020391	1668.272158	19.502426
55.646696	1670.435112	19.507443
55.912037	1665.971010	19.512461
55.760342	1665.389713	19.517479
55.840097	1662.463795	19.522496
56.220262	1665.551833	19.527514
56.079144	1657.530538	19.532531
56.076409	1661.841361	19.537549
56.052460	1667.631906	19.542567
55.988882	1662.325965	19.547584
55.894365	1662.195676	19.552602
55.662186	1664.586180	19.557619
56.033384	1656.728581	19.562637
56.456628	1670.593217	19.567655
56.600341	1656.621151	19.572672
56.271707	1664.100221	19.577690
56.343633	1676.716809	19.582707
56.556339	1674.730838	19.587725
56.675169	1696.006859	19.592743
56.931144	1687.338605	19.597760
56.937545	1683.939871	19.602778
56.812386	1684.852703	19.607795
57.095483	1685.379516	19.612813
56.769818	1692.036978	19.617831
56.857280	1683.567853	19.622848
56.758700	1685.913458	19.627866
56.592356	1681.767531	19.632883
57.477466	1680.255577	19.637901
57.143956	1681.627156	19.642919
57.256790	1678.872144	19.647936
57.340829	1675.590023	19.652954
56.924192	1680.256309	19.657971
56.970889	1672.224716	19.662989
57.302968	1681.941529	19.668007
57.330393	1688.392449	19.673024
57.428904	1699.979953	19.678042
57.392592	1702.423386	19.683059
57.717582	1705.710576	19.688077
57.680009	1714.971178	19.693095
57.902929	1707.326757	19.698112
57.943403	1695.232078	19.703130
57.904048	1698.605689	19.708147
57.720797	1707.809293	19.713165
57.557913	1710.685848	19.718183
57.928526	1707.403636	19.723200
57.690052	1713.192230	19.728218
58.074175	1721.331616	19.733235
58.505257	1728.237297	19.738253
58.376609	1738.114145	19.743271
59.025762	1723.705888	19.748288
59.108560	1703.906551	19.753306
58.561066	1700.769975	19.758323
58.483443	1695.890208	19.763341
58.670551	1699.578500	19.768359
58.831694	1681.278434	19.773376
58.458885	1686.992484	19.778394
58.336286	1684.024898	19.783411
58.594468	1696.548089	19.788429
58.744348	1705.125174	19.793447
59.037477	1711.310351	19.798464
59.126543	1716.358484	19.803482
58.995210	1716.809815	19.808499
59.374128	1709.536145	19.813517
59.226724	1712.260002	19.818535
59.253089	1709.277306	19.823552
59.159570	1707.631976	19.828570
59.127054	1712.908719	19.833587
59.543220	1709.301478	19.838605
59.338758	1711.388683	19.843623
59.125302	1717.292843	19.848640
59.326897	1714.976718	19.853658
59.026669	1722.335666	19.858675
59.229581	1708.210958	19.863693
59.230097	1724.768544	19.868711
59.646711	1719.257008	19.873728
59.830423	1737.904341	19.878746
59.545233	1745.782382	19.883763
60.014466	1737.820225	19.888781
60.155982	1741.900419	19.893799
60.009905	1747.519342	19.898816
60.236912	1741.046990	19.903834
60.107283	1746.274736	19.908851
60.332101	1732.080441	19.913869
60.064606	1742.582715	19.918887
60.624653	1733.177713	19.923904
60.719965	1734.897776	19.928922
60.368861	1728.568752	19.933939
60.369632	1734.927198	19.938957
60.228792	1735.063069	19.943975
60.312033	1734.219349	19.948992
60.378035	1733.737044	19.954010
60.122618	1735.753724	19.959027
60.134228	1731.821657	19.964045
60.555952	1740.651150	19.969063
60.800240	1750.927087	19.974080
60.894091	1747.500234	19.979098
60.748048	1762.878610	19.984115
61.141107	1748.904443	19.989133
61.174776	1752.028097	19.994151
61.401505	1753.340223	19.999168
61.153733	1753.582027	20.004186
61.064963	1752.097962	20.009203
61.329784	1749.663204	20.014221
61.114488	1757.123461	20.019239
61.177904	1754.426655	20.024256
61.397292	1764.406898	20.029274
61.612238	1774.986419	20.034291
61.764266	1777.862317	20.039309
61.790294	1777.843368	20.044327
61.606345	1780.738241	20.049344
61.832288	1783.241327	20.054362
61.806403	1784.603969	20.059379
61.965217	1782.104311	20.064397
61.951548	1782.129448	20.069415
62.051292	1777.134847	20.074432
62.193144	1778.257583	20.079450
62.284554	1776.077002	20.084467
62.294945	1776.446742	20.089485
62.169078	1779.650902	20.094503
61.869707	1783.249265	20.099520
62.147505	1789.366918	20.104538
61.884184	1782.500817	20.109555
62.389215	1795.134956	20.114573
62.476281	1817.935832	20.119591
62.563443	1816.059531	20.124608
62.581071	1811.597136	20.129626
62.218448	1811.674778	20.134643
62.544584	1808.339073	20.139661
62.685708	1824.057125	20.144679
62.778021	1815.603667	20.149696
62.878650	1803.135920	20.154714
62.891161	1816.237966	20.159731
63.381633	1826.405479	20.164749
63.266501	1830.515616	20.169767
63.404863	1833.247407	20.174784
63.388668	1795.396701	20.179802
63.224509	1811.232642	20.184819
63.519451	1824.498089	20.189837
63.141911	1818.961363	20.194855
63.144262	1832.739903	20.199872
63.592130	1817.916108	20.204890
63.600994	1831.639337	20.209907
63.520232	1819.245337	20.214925
63.493488	1830.495042	20.219943
63.850936	1828.784856	20.224960
63.803123	1819.213247	20.229978
63.732674	1831.671769	20.234995
63.888021	1824.616964	20.240013
64.285665	1834.376123	20.245031
64.263457	1846.112777	20.250048
64.409630	1838.237483	20.255066
64.219832	1846.308800	20.260083
64.492051	1840.033697	20.265101
64.326736	1841.674208	20.270119
64.193842	1844.483869	20.275136
64.498082	1842.438445	20.280154
64.332548	1846.863380	20.285171
64.522390	1850.100581	20.290189
64.481252	1840.227431	20.295207
64.635595	1848.186447	20.300224
64.395816	1842.442903	20.305242
64.356672	1852.854567	20.310259
64.718613	1857.833276	20.315277
64.994205	1878.342848	20.320295
64.758770	1878.281436	20.325312
65.154110	1867.003094	20.330330
65.166998	1881.988143	20.335347
65.416673	1871.849145	20.340365
65.279978	1866.923683	20.345383
64.994232	1869.493444	20.350400
65.606143	1868.628329	20.355418
65.315438	1865.217157	20.360435
65.494539	1874.918384	20.365453
65.459899	1862.557893	20.370471
65.373819	1872.940875	20.375488
65.995455	1889.236777	20.380506
65.935404	1890.845562	20.385523
66.126499	1894.641813	20.390541
65.980654	1869.232053	20.395559
65.770199	1876.704969	20.400576
65.921981	1870.147024	20.405594
66.060003	1884.438832	20.410611
65.892022	1888.887766	20.415629
66.161047	1894.818091	20.420647
66.131109	1896.187681	20.425664
66.378816	1886.580697	20.430682
66.445983	1900.283680	20.435699
66.146380	1893.177908	20.440717
66.517868	1893.512873	20.445735
66.158703	1889.562026	20.450752
66.307143	1895.427421	20.455770
66.288511	1918.919388	20.460787
66.736157	1910.580676	20.465805
66.707192	1926.421924	20.470823
66.973083	1919.929920	20.475840
67.235288	1903.078023	20.480858
67.264655	1918.855688	20.485875
67.090133	1912.361561	20.490893
67.171166	1921.003240	20.495911
67.532741	1913.054226	20.500928
67.524278	1905.191759	20.505946
67.338177	1908.880631	20.510963
67.385239	1901.528437	20.515981
67.392550	1907.790742	20.520999
67.560584	1908.504238	20.526016
68.000951	1905.069280	20.531034
67.675560	1911.272169	20.536051
67.767035	1916.359316	20.541069
67.868238	1911.612988	20.546087
67.896136	1912.443219	20.551104
68.231744	1908.269089	20.556122
68.273329	1904.308599	20.561139
68.217745	1897.922146	20.566157
68.018239	1904.746783	20.571175
68.051508	1910.932588	20.576192
68.610701	1917.592975	20.581210
68.623349	1924.356259	20.586227
68.426966	1920.314946	20.591245
68.487624	1919.349755	20.596263
68.471397	1926.929369	20.601280
68.556591	1930.494753	20.606298
68.327379	1938.167330	20.611315
68.486307	1926.920352	20.616333
68.881173	1928.643792	20.621351
68.544339	1926.421367	20.626368
68.837083	1927.089020	20.631386
68.838748	1933.319988	20.636403
68.988403	1927.536327	20.641421
69.281481	1949.779925	20.646439
69.130112	1945.000715	20.651456
69.354155	1951.628047	20.656474
69.636026	1955.280055	20.661491
69.649372	1935.226411	20.666509
69.754776	1925.343990	20.671527
69.263055	1927.182078	20.676544
69.625000	1919.907865	20.681562
69.434249	1941.678809	20.686579
69.284944	1947.264501	20.691597
69.662616	1950.510312	20.696615
69.791500	1945.532243	20.701632
69.721770	1942.177053	20.706650
69.815922	1956.704029	20.711667
69.703952	1949.882141	20.716685
70.044471	1946.861094	20.721703
69.699147	1963.630631	20.726720
70.118553	1973.564176	20.731738
70.503006	1972.672408	20.736755
70.384241	1978.598540	20.741773
70.414396	1980.916582	20.746791
70.325900	1983.914255	20.751808
70.638593	1976.441791	20.756826
70.552915	1982.529398	20.761843
70.490768	1983.631984	20.766861
70.693552	1977.087882	20.771879
70.160098	1990.630318	20.776896
70.607573	1998.519073	20.781914
70.998155	2007.969573	20.786931
70.678847	2006.170655	20.791949
70.901704	2007.239590	20.796967
71.425848	2008.141707	20.801984
71.389024	2010.128282	20.807002
71.136296	2005.584667	20.812019
71.244167	2006.686884	20.817037
71.563820	2011.978363	20.822055
71.554334	2030.199105	20.827072
71.926035	2032.686857	20.832090
71.620194	2030.107093	20.837107
71.821908	2036.226760	20.842125
71.881612	2026.895073	20.847143
71.818863	2035.041406	20.852160
72.239133	2030.182804	20.857178
72.286967	2022.889417	20.862195
72.118636	2025.405084	20.867213
72.706832	2026.175071	20.872231
72.402303	2024.058383	20.877248
72.424222	2020.455736	20.882266
72.608919	2015.559198	20.887283
72.418118	2016.543869	20.892301
72.287024	2023.975101	20.897319
72.276580	2020.339074	20.902336
72.673163	2019.478404	20.907354
72.408518	2023.172752	20.912371
72.131305	2023.829838	20.917389
72.630499	2024.514125	20.922407
72.629518	2045.795609	20.927424
73.104166	2044.419089	20.932442
73.232896	2044.585908	20.937459
73.295762	2045.184827	20.942477
73.219144	2042.449735	20.947495
72.965111	2050.917610	20.952512
73.256471	2038.976129	20.957530
73.651255	2038.392615	20.962547
73.307291	2046.954271	20.967565
73.636102	2043.284586	20.972583
73.774150	2046.508855	20.977600
73.429077	2039.577012	20.982618
73.338289	2042.365051	20.987635
73.404713	2048.613271	20.992653
73.826265	2056.540014	20.997671
73.845025	2068.763488	21.002688
73.646441	2068.046497	21.007706
74.064490	2072.694630	21.012723
73.657801	2075.702951	21.017741
74.139717	2074.360665	21.022759
74.139473	2082.257155	21.027776
74.468351	2091.984982	21.032794
74.489736	2110.045161	21.037811
74.793538	2100.112106	21.042829
74.761334	2096.323791	21.047847
74.751173	2102.072981	21.052864
74.877867	2090.607633	21.057882
74.997243	2092.684148	21.062899
74.995178	2091.072169	21.067917
75.058559	2083.532437	21.072935
74.885710	2086.753595	21.077952
74.908120	2087.314134	21.082970
75.308579	2087.952819	21.087987
74.888587	2090.256930	21.093005
75.220876	2088.684445	21.098023
75.087112	2094.023093	21.103040
75.368676	2096.930311	21.108058
75.570038	2110.953461	21.113075
75.332226	2108.331372	21.118093
75.607055	2103.043666	21.123111
75.727250	2107.559188	21.128128
75.880622	2104.742572	21.133146
75.733893	2103.962250	21.138163
75.963345	2099.958376	21.143181
75.805889	2104.391538	21.148199
75.918759	2115.098492	21.153216
75.964219	2122.444985	21.158234
76.227318	2118.983976	21.163251
76.262619	2133.135884	21.168269
76.632756	2122.066660	21.173287
76.740103	2122.741865	21.178304
77.023691	2112.775843	21.183322
77.213016	2109.462676	21.188339
77.442897	2110.948166	21.193357
77.400285	2111.887973	21.198375
77.024093	2096.886981	21.203392
77.227793	2080.382432	21.208410
77.649190	2077.523079	21.213427
77.248237	2081.637179	21.218445
77.488015	2076.712959	21.223463
77.290395	2072.071652	21.228480
77.019210	2075.848072	21.233498
77.192643	2073.306706	21.238515
77.182837	2077.291570	21.243533
77.407587	2075.508133	21.248551
77.351237	2097.263381	21.253568
77.105235	2100.912301	21.258586
77.729384	2103.672073	21.263603
77.649421	2109.681738	21.268621
77.680330	2101.045986	21.273639
77.503718	2102.602591	21.278656
77.755619	2107.527360	21.283674
78.045736	2125.699658	21.288691
77.909568	2135.902039	21.293709
78.155031	2143.221367	21.298727
78.085587	2140.653438	21.303744
78.083802	2136.164150	21.308762
78.407266	2135.708418	21.313779
78.267509	2135.400494	21.318797
78.669297	2157.349417	21.323815
78.302350	2160.230285	21.328832
78.646891	2165.869448	21.333850
78.647231	2167.975969	21.338867
78.436166	2171.436064	21.343885
78.802136	2164.235027	21.348903
79.071984	2189.813812	21.353920
79.204763	2194.896043	21.358938
79.715173	2189.669059	21.363955
79.257939	2184.586164	21.368973
79.569940	2181.875594	21.373991
79.812764	2185.835931	21.379008
80.018998	2188.806309	21.384026
80.126404	2177.130809	21.389043
80.013021	2184.702453	21.394061
79.959642	2176.194151	21.399079
79.705703	2166.099080	21.404096
79.780855	2176.302399	21.409114
80.148760	2182.124260	21.414131
80.064396	2181.304097	21.419149
79.744609	2174.063754	21.424167
80.000613	2177.684550	21.429184
79.863546	2184.339686	21.434202
80.129637	2192.305455	21.439219
80.025534	2220.168346	21.444237
80.364741	2211.812935	21.449255
80.569739	2211.751288	21.454272
80.526624	2217.132157	21.459290
80.788772	2206.538662	21.464307
80.837402	2212.765407	21.469325
80.963265	2219.741238	21.474343
81.187266	2233.825396	21.479360
81.168889	2237.300399	21.484378
81.247408	2235.043149	21.489395
81.142575	2237.020936	21.494413
81.669948	2228.184805	21.499431
81.177674	2232.020119	21.504448
81.393666	2239.836589	21.509466
81.781181	2228.220993	21.514483
81.563797	2235.113920	21.519501
81.628156	2231.003408	21.524519
81.955007	2221.748552	21.529536
81.993890	2224.341328	21.534554
81.853630	2222.336063	21.539571
81.758457	2225.624307	21.544589
81.944759	2228.129862	21.549607
81.896572	2227.701146	21.554624
81.857066	2243.560938	21.559642
82.247270	2254.861679	21.564659
82.348526	2257.413050	21.569677
82.627331	2258.392066	21.574695
82.632883	2256.280954	21.579712
82.546204	2265.100604	21.584730
82.366863	2253.608422	21.589747
82.590024	2261.607032	21.594765
82.829903	2276.174015	21.599783
83.030809	2282.316726	21.604800
82.738489	2280.067481	21.609818
83.408992	2275.200358	21.614835
82.979925	2280.174002	21.619853
83.094258	2270.272620	21.624871
83.432834	2275.155308	21.629888
83.615490	2269.692678	21.634906
83.789004	2260.907451	21.639923
83.310808	2270.389695	21.644941
83.747604	2287.166234	21.649959
83.654495	2293.458878	21.654976
83.676398	2297.243675	21.659994
83.920661	2295.357205	21.665011
83.796180	2307.472365	21.670029
83.739536	2302.680291	21.675047
83.861930	2310.009104	21.680064
84.062961	2319.645779	21.685082
84.249340	2320.813372	21.690099
84.358333	2328.820001	21.695117
84.431361	2323.842846	21.700135
84.627467	2324.995517	21.705152
84.755908	2326.844086	21.710170
84.944453	2318.596806	21.715187
84.951897	2324.660266	21.720205
84.773648	2315.188575	21.725223
85.266498	2330.465664	21.730240
85.150701	2339.234942	21.735258
85.187826	2338.359215	21.740275
85.159736	2351.643624	21.745293
85.568649	2339.519545	21.750311
85.654049	2348.923762	21.755328
85.864554	2345.437265	21.760346
85.931049	2341.773943	21.765363
85.533266	2333.686229	21.770381
85.718605	2340.112255	21.775399
85.916111	2345.278607	21.780416
85.790310	2350.803284	21.785434
86.193793	2337.096693	21.790451
85.944937	2341.363589	21.795469
86.339129	2336.826824	21.800487
86.219971	2342.099520	21.805504
85.966581	2345.876317	21.810522
86.520920	2335.468959	21.815539
86.055064	2337.280158	21.820557
86.270356	2337.583413	21.825575
86.159857	2359.180933	21.830592
86.442282	2370.635816	21.835610
86.903739	2366.011231	21.840627
86.192819	2371.080979	21.845645
86.682847	2373.466546	21.850663
86.906142	2394.768621	21.855680
87.128081	2397.270096	21.860698
87.500926	2388.278385	21.865715
87.394201	2389.433732	21.870733
87.499798	2391.548670	21.875751
87.700743	2390.282629	21.880768
87.449882	2385.314628	21.885786
87.691596	2383.618906	21.890803
87.462760	2385.765937	21.895821
87.456801	2392.508022	21.900839
88.213637	2389.369370	21.905856
88.039826	2416.106356	21.910874
88.224114	2408.180630	21.915891
88.715680	2407.020052	21.920909
88.274166	2412.424410	21.925927
88.289640	2403.867238	21.930944
88.682451	2413.701502	21.935962
88.789404	2401.494167	21.940979
88.568346	2410.256676	21.945997
88.611440	2404.018659	21.951015
88.916393	2399.750172	21.956032
88.867955	2407.058296	21.961050
89.222712	2398.488711	21.966067
88.908599	2396.111562	21.971085
89.181251	2397.845114	21.976103
89.513746	2403.377745	21.981120
89.206493	2402.873922	21.986138
89.297725	2396.084705	21.991155
89.201041	2427.418773	21.996173
89.486590	2430.469369	22.001191
89.673395	2433.456268	22.006208
89.876524	2438.701202	22.011226
89.985534	2427.059070	22.016243
89.961636	2429.082969	22.021261
89.714954	2428.818834	22.026279
89.790258	2427.759245	22.031296
89.754120	2429.926681	22.036314
90.102007	2435.449003	22.041331
90.229187	2442.898255	22.046349
90.368822	2447.424942	22.051367
90.787373	2435.444765	22.056384
90.391989	2448.237227	22.061402
90.544618	2452.705996	22.066419
90.451091	2454.718192	22.071437
90.354823	2448.614861	22.076455
90.555133	2464.265961	22.081472
90.577601	2478.238550	22.086490
91.047108	2471.254470	22.091507
91.060850	2483.726080	22.096525
90.965771	2485.635485	22.101543
91.409093	2477.839102	22.106560
91.005336	2498.407545	22.111578
91.592373	2503.514196	22.116595
91.944287	2498.036289	22.121613
91.672068	2500.879304	22.126631
91.765141	2497.436669	22.131648
91.422418	2510.181457	22.136666
91.821104	2500.087483	22.141683
92.035251	2514.407102	22.146701
92.039127	2525.878210	22.151719
92.454380	2522.583985	22.156736
92.407697	2533.364673	22.161754
92.730759	2528.664571	22.166771
92.651063	2531.801751	22.171789
92.951855	2531.397607	22.176807
92.998242	2521.399915	22.181824
92.797002	2523.434016	22.186842
93.184925	2517.384804	22.191859
92.977269	2521.779688	22.196877
92.934148	2521.029228	22.201895
93.516416	2513.745548	22.206912
93.193351	2523.690113	22.211930
93.010828	2516.995623	22.216947
93.187661	2520.376637	22.221965
93.198763	2540.529738	22.226983
93.482854	2544.574839	22.232000
93.322490	2549.700009	22.237018
93.708692	2536.445917	22.242035
93.800197	2547.650574	22.247053
93.781353	2571.460623	22.252071
94.082137	2573.527944	22.257088
94.272434	2568.779781	22.262106
94.239843	2571.704158	22.267123
94.337978	2574.091686	22.272141
94.542508	2569.862762	22.277159
94.769541	2565.892972	22.282176
94.310921	2576.327209	22.287194
94.657813	2568.653132	22.292211
94.763883	2568.832225	22.297229
94.800641	2586.919649	22.302247
94.933941	2591.237371	22.307264
95.012279	2601.535658	22.312282
95.334884	2591.402626	22.317299
95.455367	2591.828770	22.322317
95.509017	2591.684281	22.327335
95.603448	2584.962113	22.332352
95.412364	2597.367373	22.337370
95.356985	2590.651001	22.342387
95.562234	2585.336463	22.347405
95.585854	2590.202624	22.352423
95.625929	2594.677586	22.357440
95.826382	2612.578473	22.362458
95.920596	2613.546049	22.367475
96.466225	2617.627337	22.372493
96.332016	2618.698986	22.377511
96.407829	2609.513810	22.382528
96.802042	2608.671581	22.387546
96.837417	2606.771188	22.392563
97.072446	2601.734281	22.397581
96.645121	2611.362803	22.402599
96.789940	2601.911772	22.407616
96.668985	2603.759245	22.412634
96.733545	2606.715332	22.417651
97.154443	2610.840893	22.422669
96.968223	2631.823977	22.427687
97.276259	2630.274970	22.432704
97.209259	2639.938082	22.437722
97.435926	2627.940366	22.442739
97.487117	2626.614807	22.447757
97.554128	2634.447383	22.452775
97.717503	2633.689946	22.457792
97.957857	2653.714615	22.462810
97.637177	2653.894113	22.467827
97.843816	2655.067157	22.472845
97.920539	2661.679765	22.477863
98.318384	2651.662121	22.482880
98.211255	2663.232059	22.487898
97.950625	2669.355716	22.492915
98.486678	2675.688209	22.497933
98.323634	2686.092694	22.502951
98.977434	2683.340902	22.507968
98.749953	2672.361845	22.512986
98.885466	2679.467720	22.518003
98.930423	2672.865885	22.523021
99.150780	2694.972769	22.528039
99.902821	2693.065846	22.533056
99.539021	2698.450835	22.538074
99.731552	2691.558015	22.543091
100.015114	2676.795742	22.548109
99.825368	2679.803409	22.553127
99.745810	2672.909937	22.558144
99.915286	2675.181489	22.563162
100.076256	2690.341979	22.568179
100.323869	2690.786396	22.573197
99.805446	2699.780561	22.578215
100.291811	2688.160639	22.583232
100.363628	2697.302164	22.588250
100.512136	2696.990735	22.593267
100.489121	2689.085329	22.598285
100.583908	2695.324585	22.603303
100.870033	2691.404333	22.608320
100.477021	2691.969786	22.613338
100.615802	2694.125886	22.618355
100.737218	2687.011577	22.623373
100.622012	2708.362585	22.628391
100.857442	2705.183522	22.633408
101.164455	2716.240674	22.638426
101.143548	2721.091954	22.643443
101.350715	2719.017845	22.648461
101.109983	2725.656720	22.653479
101.493569	2737.257802	22.658496
101.470962	2748.365180	22.663514
101.412006	2751.971846	22.668531
101.932598	2740.034932	22.673549
101.679859	2751.367795	22.678567
102.154620	2759.794587	22.683584
102.099484	2773.563519	22.688602
102.174881	2773.601199	22.693619
102.513500	2763.769123	22.698637
103.027280	2764.613955	22.703655
102.834844	2748.377912	22.708672
102.698251	2762.868549	22.713690
102.695761	2763.127098	22.718707
102.897731	2760.342725	22.723725
102.649810	2776.643790	22.728743
103.240702	2771.081265	22.733760
103.343474	2788.536998	22.738778
103.212795	2796.520749	22.743795
103.834634	2790.697636	22.748813
103.387015	2797.913863	22.753831
103.397303	2789.855210	22.758848
103.633998	2795.808369	22.763866
103.654173	2791.173003	22.768883
103.931402	2793.380195	22.773901
104.131049	2813.751387	22.778919
104.176329	2807.888845	22.783936
104.237216	2806.600268	22.788954
104.033446	2806.308042	22.793971
104.473535	2803.477037	22.798989
104.467960	2808.409282	22.804007
104.358981	2803.143987	22.809024
104.173209	2824.660592	22.814042
104.373254	2834.612408	22.819059
104.573385	2833.392870	22.824077
104.828136	2853.709708	22.829095
105.208312	2854.542027	22.834112
105.549288	2862.010104	22.839130
105.619911	2870.510845	22.844147
105.711039	2860.214743	22.849165
105.717257	2857.094223	22.854183
105.735136	2862.074661	22.859200
106.003207	2857.306138	22.864218
105.966873	2858.535249	22.869235
106.326731	2849.667253	22.874253
105.766444	2860.706282	22.879271
106.335412	2855.252628	22.884288
106.634398	2845.363889	22.889306
106.408704	2850.061443	22.894323
106.695433	2847.700104	22.899341
106.418702	2857.333089	22.904359
106.845685	2849.832521	22.909376
106.873190	2851.270914	22.914394
106.658186	2850.814504	22.919411
106.867351	2866.585764	22.924429
106.822769	2874.178257	22.929447
106.805315	2881.157595	22.934464
107.006092	2881.417557	22.939482
106.971931	2885.489905	22.944499
107.150881	2889.373310	22.949517
107.489975	2904.607878	22.954535
107.519318	2900.808752	22.959552
107.749645	2899.243793	22.964570
107.913836	2908.311725	22.969587
108.282388	2918.181667	22.974605
108.049115	2931.905213	22.979623
108.115549	2936.938503	22.984640
108.650088	2928.450855	22.989658
108.501036	2933.586940	22.994675
108.594995	2920.231222	22.999693
108.532922	2928.555719	23.004711
108.761815	2927.938849	23.009728
109.187298	2919.039895	23.014746
108.914740	2923.569531	23.019763
109.293014	2934.664256	23.024781
109.362059	2956.602947	23.029799
109.434921	2949.444337	23.034816
109.336064	2947.242795	23.039834
109.718376	2953.447325	23.044851
109.821491	2943.397822	23.049869
109.611041	2945.851925	23.054887
109.701420	2944.055202	23.059904
109.954491	2943.620116	23.064922
110.018178	2958.952147	23.069939
110.381405	2970.763541	23.074957
110.439593	2980.932372	23.079975
110.446603	2975.385791	23.084992
110.390429	2978.452454	23.090010
110.602304	2977.857174	23.095027
110.603178	2973.018736	23.100045
110.566851	2980.371625	23.105063
110.678219	2984.813314	23.110080
110.757141	2995.469694	23.115098
110.944141	3000.660769	23.120115
110.939738	2992.774255	23.125133
111.120409	2996.511892	23.130151
111.292151	3010.098559	23.135168
111.692850	3020.357537	23.140186
111.596623	3027.665725	23.145203
111.759856	3016.105726	23.150221
111.983098	3021.604887	23.155239
112.132757	3014.661330	23.160256
112.204306	3025.446340	23.165274
111.973565	3026.733997	23.170291
112.406576	3013.807109	23.175309
112.147926	3015.660071	23.180327
112.467998	3035.195079	23.185344
112.690182	3032.482947	23.190362
112.803957	3044.323953	23.195379
112.731093	3051.817215	23.200397
112.683153	3048.541674	23.205415
112.702134	3044.490873	23.210432
113.056965	3045.720555	23.215450
113.185924	3072.596889	23.220467
113.687928	3063.123216	23.225485
113.307861	3064.876766	23.230503
113.088524	3069.741711	23.235520
113.629924	3068.067348	23.240538
113.792630	3085.533545	23.245555
113.938950	3089.787197	23.250573
114.151646	3094.091623	23.255591
114.381159	3092.549586	23.260608
114.529009	3079.760933	23.265626
114.376844	3087.150439	23.270643
114.813598	3091.879308	23.275661
114.950337	3089.790420	23.280679
114.647520	3087.385394	23.285696
114.762209	3080.665275	23.290714
114.925934	3105.177849	23.295731
115.056355	3107.754612	23.300749
115.331463	3113.211714	23.305767
115.309947	3115.301404	23.310784
115.395545	3110.937900	23.315802
115.307312	3117.173484	23.320819
115.600858	3114.328819	23.325837
115.848769	3114.366523	23.330855
116.300989	3132.481982	23.335872
116.414297	3124.174665	23.340890
116.547518	3127.418825	23.345907
116.368288	3130.409961	23.350925
116.833461	3125.221333	23.355943
116.557088	3131.826742	23.360960
116.906193	3128.250312	23.365978
116.839015	3128.351632	23.370995
116.891425	3127.644117	23.376013
116.763211	3120.828987	23.381031
116.483205	3129.257571	23.386048
117.006837	3128.755739	23.391066
117.067979	3147.950677	23.396083
117.340616	3139.978217	23.401101
117.583786	3153.339668	23.406119
117.590951	3159.829868	23.411136
117.915653	3158.872838	23.416154
117.983781	3163.802102	23.421171
118.108006	3148.773713	23.426189
118.278082	3148.945755	23.431207
118.099075	3149.140422	23.436224
118.157281	3151.923004	23.441242
118.071894	3152.617194	23.446259
118.104494	3167.200031	23.451277
118.316917	3174.382773	23.456295
118.143660	3172.001124	23.461312
118.782598	3179.646828	23.466330
118.390762	3205.344709	23.471347
118.504504	3203.744819	23.476365
119.164915	3210.763323	23.481383
118.838821	3212.932272	23.486400
119.166487	3224.667736	23.491418
119.568068	3238.535763	23.496435
119.943064	3238.692436	23.501453
120.179180	3229.616610	23.506471
120.156336	3231.262086	23.511488
120.439439	3231.985622	23.516506
120.256704	3234.142728	23.521523
120.441216	3227.173061	23.526541
120.643248	3225.563024	23.531559
120.210126	3226.680019	23.536576
120.805913	3217.500437	23.541594
120.696279	3235.295785	23.546611
120.680603	3248.168411	23.551629
120.948859	3248.073079	23.556647
120.796710	3256.655979	23.561664
121.093552	3246.381080	23.566682
120.790616	3258.859798	23.571699
121.050017	3267.272459	23.576717
122.038492	3257.062686	23.581735
121.971070	3264.892652	23.586752
121.900164	3260.820725	23.591770
122.444773	3264.156644	23.596787
122.289143	3264.511990	23.601805
122.734587	3261.022429	23.606823
122.379643	3263.939348	23.611840
122.796841	3256.614767	23.616858
122.537731	3261.588378	23.621875
122.614848	3256.583510	23.626893
123.004968	3253.472486	23.631911
122.911792	3268.416090	23.636928
123.156088	3248.180648	23.641946
122.981706	3270.810741	23.646963
122.914103	3275.232286	23.651981
122.992337	3286.943070	23.656999
122.980064	3287.297583	23.662016
123.248531	3296.707046	23.667034
123.287495	3305.331871	23.672051
123.087190	3309.561410	23.677069
123.875607	3317.787484	23.682087
123.959539	3327.000629	23.687104
124.082684	3330.797083	23.692122
124.167138	3341.674664	23.697139
124.598653	3338.438242	23.702157
124.522064	3335.611651	23.707175
124.328176	3338.706640	23.712192
124.749301	3334.031555	23.717210
125.084318	3349.378155	23.722227
124.869174	3360.133610	23.727245
125.660311	3364.254633	23.732263
125.358413	3362.872821	23.737280
125.532452	3352.145451	23.742298
125.678403	3353.295980	23.747315
125.784348	3352.476082	23.752333
125.881250	3350.630286	23.757351
125.537486	3367.274527	23.762368
125.854228	3348.955431	23.767386
125.836930	3371.648733	23.772403
125.747816	3376.754963	23.777421
126.092304	3385.118726	23.782439
126.124966	3391.021282	23.787456
126.384341	3401.944960	23.792474
126.412405	3414.813905	23.797491
126.387886	3418.996566	23.802509
126.908888	3423.767177	23.807527
126.825995	3439.081393	23.812544
127.038459	3438.860442	23.817562
127.495936	3444.162728	23.822579
127.402017	3435.683753	23.827597
127.427274	3435.625594	23.832615
127.787274	3457.310185	23.837632
127.736213	3456.300565	23.842650
127.976935	3457.447791	23.847667
127.679910	3464.627739	23.852685
128.154361	3465.077707	23.857703
128.240285	3487.230829	23.862720
128.731436	3490.606792	23.867738
128.944311	3481.178956	23.872755
128.754977	3499.453022	23.877773
129.125236	3489.644524	23.882791
128.940727	3495.699746	23.887808
129.010107	3485.241479	23.892826
128.937439	3493.652156	23.897843
129.330643	3509.213839	23.902861
129.938999	3503.144026	23.907879
129.470423	3517.432686	23.912896
129.612548	3518.251876	23.917914
129.784462	3515.661736	23.922931
130.371819	3527.912192	23.927949
130.278488	3533.265366	23.932967
130.136804	3544.384470	23.937984
130.620819	3536.492942	23.943002
130.781408	3535.109740	23.948019
130.596961	3542.293014	23.953037
130.872738	3532.060608	23.958055
130.687866	3537.433887	23.963072
130.706215	3534.345115	23.968090
130.868996	3543.139130	23.973107
130.610893	3553.925962	23.978125
131.372342	3549.083268	23.983143
131.362037	3555.046232	23.988160
131.804339	3562.499303	23.993178
131.861415	3586.640302	23.998195
131.888344	3579.141798	24.003213
132.286759	3573.321760	24.008231
132.197975	3581.602901	24.013248
132.418591	3580.089767	24.018266
132.481778	3579.017082	24.023283
132.462958	3579.472550	24.028301
132.497767	3569.852004	24.033319
132.902384	3600.046681	24.038336
133.200301	3601.684318	24.043354
133.070382	3603.563236	24.048371
133.003665	3611.544310	24.053389
133.223274	3601.740094	24.058407
133.133914	3617.029567	24.063424
133.338123	3623.195135	24.068442
133.751724	3628.737334	24.073459
133.788504	3638.221720	24.078477
133.840496	3629.568331	24.083495
134.175120	3625.909921	24.088512
134.530009	3638.185738	24.093530
134.550598	3651.338490	24.098547
134.363372	3657.817428	24.103565
134.854847	3657.054825	24.108583
134.520103	3661.225662	24.113600
134.889669	3651.264559	24.118618
134.739241	3668.260622	24.123635
135.063968	3686.965061	24.128653
135.538037	3686.807020	24.133671
135.407137	3695.077633	24.138688
135.485451	3683.360734	24.143706
135.600742	3685.574222	24.148723
135.754596	3694.403578	24.153741
136.199159	3697.228498	24.158759
136.500143	3704.048895	24.163776
136.693292	3696.297273	24.168794
136.867060	3706.866678	24.173811
136.322185	3706.631178	24.178829
136.552261	3696.932214	24.183847
136.894440	3702.701372	24.188864
137.004091	3706.097311	24.193882
137.210007	3723.187655	24.198899
137.255840	3730.002336	24.203917
137.119224	3733.432042	24.208935
137.100902	3734.358640	24.213952
137.249399	3743.944853	24.218970
137.631376	3753.237395	24.223987
137.744909	3758.116355	24.229005
137.947607	3761.673681	24.234023
137.686373	3758.774184	24.239040
138.190302	3767.390435	24.244058
138.256403	3781.542963	24.249075
138.324064	3788.424203	24.254093
138.533194	3787.147303	24.259111
138.708638	3793.953934	24.264128
138.841942	3786.061556	24.269146
139.026059	3795.683029	24.274163
139.031961	3810.225925	24.279181
139.208216	3807.212608	24.284199
139.102468	3809.280429	24.289216
139.516342	3813.208437	24.294234
139.393266	3815.755734	24.299251
139.749706	3836.749200	24.304269
139.745940	3831.576102	24.309287
139.932895	3843.035572	24.314304
140.270202	3848.837031	24.319322
140.529553	3851.248625	24.324339
140.513532	3853.597141	24.329357
140.704561	3851.522304	24.334375
140.698257	3852.649164	24.339392
140.911089	3860.496907	24.344410
141.047133	3863.183828	24.349427
141.317982	3883.770146	24.354445
141.432205	3877.789985	24.359463
141.502242	3884.755064	24.364480
141.518207	3876.688615	24.369498
142.046489	3881.565992	24.374515
141.941065	3889.274911	24.379533
142.660259	3898.232153	24.384551
142.418325	3900.442846	24.389568
142.592195	3899.822914	24.394586
142.857103	3892.594677	24.399603
142.487103	3909.648842	24.404621
142.853786	3888.135135	24.409639
143.063340	3893.590399	24.414656
142.975935	3905.907071	24.419674
143.459112	3914.085402	24.424691
143.726495	3930.111274	24.429709
143.739303	3919.463479	24.434727
143.631579	3931.882533	24.439744
143.716196	3929.033269	24.444762
143.817827	3927.406126	24.449779
143.878227	3942.838046	24.454797
144.191208	3945.010613	24.459815
144.199023	3949.291322	24.464832
144.195185	3950.363516	24.469850
144.874335	3957.417162	24.474867
144.606354	3972.082554	24.479885
144.656116	3979.087098	24.484903
144.922547	3979.376736	24.489920
145.056920	3977.236182	24.494938
145.417098	3977.861725	24.499955
145.321450	4003.893731	24.504973
145.428500	4003.878383	24.509991
145.394227	4003.196448	24.515008
145.672532	4011.271406	24.520026
146.099514	4024.829335	24.525043
145.907914	4035.454087	24.530061
146.490795	4033.732893	24.535079
146.677575	4040.563006	24.540096
146.174429	4038.408452	24.545114
146.454276	4020.830726	24.550131
146.289083	4050.358840	24.555149
146.738653	4048.106659	24.560167
147.023771	4053.227400	24.565184
146.826966	4071.737795	24.570202
147.460630	4077.769001	24.575219
147.479958	4079.334687	24.580237
147.775627	4078.291766	24.585255
147.920760	4089.312056	24.590272
148.113630	4112.694372	24.595290
148.550879	4103.342858	24.600307
148.334625	4118.177935	24.605325
148.502572	4115.498644	24.610343
148.799698	4102.431207	24.615360
148.633355	4109.151667	24.620378
149.274428	4115.015720	24.625395
149.194196	4126.278079	24.630413
149.582328	4126.298941	24.635431
149.584846	4133.698134	24.640448
149.797274	4134.814527	24.645466
150.029062	4120.100757	24.650483
150.215107	4125.598404	24.655501
150.332559	4119.646737	24.660519
150.672144	4113.446467	24.665536
150.475597	4124.193220	24.670554
150.591991	4114.935338	24.675571
150.322136	4121.376519	24.680589
150.659034	4114.336510	24.685607
150.852223	4138.469303	24.690624
150.886005	4141.458143	24.695642
150.930185	4133.601817	24.700659
150.707441	4153.356247	24.705677
151.341986	4167.899172	24.710695
151.374858	4163.674352	24.715712
151.386907	4171.361541	24.720730
151.565895	4183.871187	24.725747
151.640350	4202.564272	24.730765
151.872200	4197.580040	24.735783
152.020701	4209.641443	24.740800
152.141089	4233.612930	24.745818
152.653192	4234.838886	24.750835
152.443286	4235.136038	24.755853
153.012499	4250.483221	24.760871
153.242450	4256.973786	24.765888
153.265535	4260.213734	24.770906
153.592288	4258.736318	24.775923
153.284366	4267.611327	24.780941
153.844761	4269.322048	24.785959
154.254599	4280.663723	24.790976
154.368701	4290.841070	24.795994
154.708238	4283.500835	24.801011
154.341954	4288.738108	24.806029
154.183364	4281.245225	24.811047
154.760963	4277.762683	24.816064
154.721978	4276.850988	24.821082
154.739303	4266.724578	24.826099
154.749752	4280.519081	24.831117
155.074637	4289.242073	24.836135
155.235401	4298.686665	24.841152
155.124327	4306.347928	24.846170
155.376216	4299.242718	24.851187
155.555115	4321.717403	24.856205
155.725970	4339.194026	24.861223
155.881233	4334.879628	24.866240
155.852957	4341.064475	24.871258
156.060891	4350.233320	24.876275
156.431428	4356.076886	24.881293
156.488692	4360.314430	24.886311
156.845033	4363.118937	24.891328
156.849347	4376.388216	24.896346
157.183005	4381.647658	24.901363
157.436798	4377.802137	24.906381
157.597946	4374.393052	24.911399
157.930444	4391.234282	24.916416
158.152503	4403.556311	24.921434
158.234608	4397.160970	24.926451
158.115323	4404.985651	24.931469
158.252024	4401.794437	24.936487
158.572216	4388.182615	24.941504
158.383118	4397.445473	24.946522
158.823189	4407.191745	24.951539
159.026113	4416.595076	24.956557
159.283298	4429.710016	24.961575
159.055755	4417.433187	24.966592
159.204096	4423.612723	24.971610
159.714924	4437.860182	24.976627
159.784754	4446.382420	24.981645
159.789468	4449.226487	24.986663
159.831785	4451.561864	24.991680
160.044715	4455.626719	24.996698
160.313180	4468.839018	25.001715
160.429718	4476.560055	25.006733
160.455436	4480.723208	25.011751
160.722606	4477.486788	25.016768
161.059656	4493.580054	25.021786
161.374587	4496.541448	25.026803
161.262467	4511.918082	25.031821
161.406960	4498.153233	25.036839
161.620477	4498.877709	25.041856
161.597135	4509.860668	25.046874
162.125178	4520.134235	25.051891
162.156794	4526.408734	25.056909
161.905102	4533.529261	25.061927
162.232407	4530.021273	25.066944
162.265236	4533.230620	25.071962
162.388113	4550.990488	25.076979
162.303241	4554.542724	25.081997
162.665016	4561.412836	25.087015
162.813609	4577.036688	25.092032
162.843150	4584.000689	25.097050
163.255746	4577.705196	25.102067
163.364486	4586.198498	25.107085
163.452877	4609.566009	25.112103
163.761892	4610.452272	25.117120
164.017907	4611.852046	25.122138
164.380676	4614.768863	25.127155
164.432647	4639.304969	25.132173
164.817840	4643.848260	25.137191
165.209731	4633.333037	25.142208
164.681042	4637.854465	25.147226
164.883082	4638.790041	25.152243
165.379291	4646.988737	25.157261
165.664705	4652.951414	25.162279
165.761016	4656.955462	25.167296
165.847720	4653.419723	25.172314
166.325442	4650.351092	25.177331
166.108836	4664.448848	25.182349
166.126719	4655.934033	25.187367
166.462784	4660.037528	25.192384
166.242476	4674.834476	25.197402
166.381760	4675.107429	25.202419
167.087702	4687.162165	25.207437
167.110833	4700.158110	25.212455
167.386707	4707.078175	25.217472
167.342773	4716.114332	25.222490
167.777916	4706.367851	25.227507
167.726168	4716.194318	25.232525
167.623144	4720.237245	25.237543
168.375712	4726.719433	25.242560
168.486476	4740.746186	25.247578
168.356264	4735.650359	25.252595
168.665077	4744.225926	25.257613
169.047494	4737.033613	25.262631
169.055139	4755.079579	25.267648
168.842374	4759.669467	25.272666
169.169282	4762.925596	25.277683
169.229713	4758.689918	25.282701
169.707260	4769.408334	25.287719
169.919508	4775.759560	25.292736
169.694084	4793.388016	25.297754
170.011493	4790.172628	25.302771
170.565679	4775.618429	25.307789
170.466273	4785.224394	25.312807
170.617615	4795.470892	25.317824
170.726100	4814.179783	25.322842
170.745669	4803.110954	25.327859
170.723232	4806.583279	25.332877
170.971424	4834.586924	25.337895
171.437358	4833.448365	25.342912
171.393193	4840.377036	25.347930
171.595132	4848.847763	25.352947
171.897991	4849.270078	25.357965
171.900286	4859.462498	25.362983
171.938713	4861.559400	25.368000
172.188544	4873.580806	25.373018
172.303550	4865.225822	25.378035
172.808665	4883.297265	25.383053
172.395041	4893.894307	25.388071
172.814220	4886.262582	25.393088
172.935755	4898.707261	25.398106
173.328720	4912.382367	25.403123
173.703674	4911.607609	25.408141
173.582901	4921.665498	25.413159
174.376709	4913.594047	25.418176
174.039385	4922.748697	25.423194
174.254189	4946.106816	25.428211
174.629050	4950.389088	25.433229
174.618873	4958.608906	25.438247
174.605866	4949.019470	25.443264
174.855846	4960.822217	25.448282
174.967429	4971.160928	25.453299
175.262772	4976.844443	25.458317
175.307169	4979.718474	25.463335
175.372941	4979.671159	25.468352
175.897090	5004.525166	25.473370
175.883746	4999.128183	25.478387
176.184637	4998.863223	25.483405
176.079026	5015.409196	25.488423
176.419467	5025.198515	25.493440
176.697365	5030.309740	25.498458
176.735997	5038.237814	25.503475
177.307526	5047.784971	25.508493
176.970239	5063.010052	25.513511
177.088063	5068.806084	25.518528
177.148839	5065.280675	25.523546
177.366580	5082.970204	25.528563
177.808947	5078.287260	25.533581
177.699793	5100.200138	25.538599
178.245011	5111.560212	25.543616
178.337095	5121.983170	25.548634
178.336071	5123.701691	25.553651
179.020234	5130.796027	25.558669
178.897231	5149.136300	25.563687
179.377720	5130.897458	25.568704
179.582400	5151.194790	25.573722
179.481555	5139.644548	25.578739
180.012292	5149.630189	25.583757
179.936355	5170.319233	25.588775
180.204463	5164.493393	25.593792
180.197677	5171.258915	25.598810
180.549978	5160.638703	25.603827
180.778784	5170.166629	25.608845
181.293037	5181.809411	25.613863
181.273165	5181.391826	25.618880
181.548831	5180.079029	25.623898
181.460123	5167.324707	25.628915
181.809559	5172.101231	25.633933
181.357193	5181.196495	25.638951
181.885564	5171.453730	25.643968
181.749355	5184.016055	25.648986
181.843177	5178.305323	25.654003
182.331547	5199.706905	25.659021
182.077165	5205.932884	25.664039
182.168551	5201.456912	25.669056
182.090715	5228.705314	25.674074
182.255294	5237.331701	25.679092
182.658832	5243.625097	25.684109
182.655791	5271.724699	25.689127
183.255617	5281.408325	25.694144
183.687691	5291.123422	25.699162
183.758117	5301.219531	25.704180
183.916070	5302.699521	25.709197
184.135592	5318.935948	25.714215
184.356011	5327.676217	25.719232
184.623346	5337.767707	25.724250
185.253661	5334.418137	25.729268
185.465032	5347.047917	25.734285
185.388538	5356.298929	25.739303
185.494382	5343.426110	25.744320
185.759065	5352.629806	25.749338
185.745534	5341.375460	25.754356
186.354087	5367.323566	25.759373
186.423902	5364.841435	25.764391
186.697189	5359.783337	25.769408
186.703089	5364.515565	25.774426
187.127317	5368.946653	25.779444
187.176109	5360.257354	25.784461
187.148135	5362.292534	25.789479
187.317269	5375.077766	25.794496
187.238421	5384.211160	25.799514
187.104378	5391.028540	25.804532
187.482310	5401.764091	25.809549
187.478499	5424.893478	25.814567
187.699486	5430.323893	25.819584
187.950399	5444.435970	25.824602
188.203029	5453.492957	25.829620
188.602127	5450.579103	25.834637
188.653646	5475.820810	25.839655
188.677080	5474.858179	25.844672
189.100293	5489.432972	25.849690
189.040576	5501.499523	25.854708
189.751827	5509.383556	25.859725
189.687655	5539.250219	25.864743
189.889866	5530.163443	25.869760
190.213069	5540.342936	25.874778
190.429277	5557.934149	25.879796
190.954123	5557.269214	25.884813
190.881165	5566.069772	25.889831
190.913384	5566.532111	25.894848
190.747218	5561.853199	25.899866
191.359351	5568.908098	25.904884
191.617449	5584.422726	25.909901
191.673173	5595.928878	25.914919
191.839806	5589.183603	25.919936
192.327275	5587.451497	25.924954
192.269922	5602.074694	25.929972
192.545266	5600.057770	25.934989
192.739437	5612.980833	25.940007
192.631041	5609.171498	25.945024
192.912763	5617.137443	25.950042
193.124735	5622.736159	25.955060
193.302492	5637.201534	25.960077
193.201850	5637.604809	25.965095
193.812598	5650.459131	25.970112
194.090469	5660.579847	25.975130
193.898707	5670.120075	25.980148
194.250466	5670.198677	25.985165
194.372923	5687.418695	25.990183
194.559851	5694.129970	25.995200
195.408738	5698.570560	26.000218
195.057010	5701.227013	26.005236
195.653303	5702.845653	26.010253
195.860423	5712.118546	26.015271
195.981011	5700.246969	26.020288
196.151627	5699.754155	26.025306
196.230392	5713.188214	26.030324
196.666951	5711.262801	26.035341
196.749143	5723.187322	26.040359
196.740520	5731.508027	26.045376
197.144702	5731.981093	26.050394
197.171195	5731.298044	26.055412
197.576128	5724.496621	26.060429
197.498936	5747.074893	26.065447
197.790683	5749.689349	26.070464
198.040425	5754.554341	26.075482
197.928649	5765.682935	26.080500
198.500353	5778.790637	26.085517
198.587011	5788.862464	26.090535
198.618027	5793.606560	26.095552
198.667313	5786.630500	26.100570
198.309311	5803.691222	26.105588
199.085251	5810.639875	26.110605
198.989483	5824.525139	26.115623
199.168083	5840.183313	26.120640
199.626626	5839.344049	26.125658
199.433521	5869.324771	26.130676
200.074379	5873.440603	26.135693
200.553870	5901.032540	26.140711
200.871893	5903.138517	26.145728
200.909652	5913.629704	26.150746
201.082800	5912.993288	26.155764
201.210951	5908.087961	26.160781
200.991485	5928.890639	26.165799
201.512266	5924.626871	26.170816
201.733195	5925.271565	26.175834
201.812525	5935.398159	26.180852
202.193586	5940.230477	26.185869
202.460494	5948.570320	26.190887
202.615295	5952.404896	26.195904
202.741681	5953.860875	26.200922
202.898680	5975.240886	26.205940
202.965263	5981.353076	26.210957
203.372559	5984.504614	26.215975
203.413621	5987.535155	26.220992
203.676817	5994.136849	26.226010
203.806487	6016.403248	26.231028
203.871190	6010.629963	26.236045
204.069812	6019.292295	26.241063
204.256244	6031.689033	26.246080
204.366272	6045.653417	26.251098
204.771594	6061.625797	26.256116
204.998997	6057.382012	26.261133
205.278896	6074.289422	26.266151
205.408105	6080.066730	26.271168
206.122113	6071.629735	26.276186
205.989165	6086.584107	26.281204
206.307261	6093.511474	26.286221
206.504195	6108.420358	26.291239
206.756418	6098.500718	26.296256
206.821035	6107.594377	26.301274
207.156756	6125.887118	26.306292
207.447582	6129.929796	26.311309
207.653355	6127.766538	26.316327
207.593000	6143.245191	26.321344
207.995220	6147.970349	26.326362
207.653832	6166.836861	26.331380
208.141848	6160.681320	26.336397
208.564164	6174.256151	26.341415
208.818515	6183.222834	26.346432
209.147053	6181.707190	26.351450
208.844568	6188.287429	26.356468
209.468672	6195.753001	26.361485
209.655808	6212.008165	26.366503
209.266366	6221.402446	26.371520
209.806640	6220.808200	26.376538
209.935277	6249.563729	26.381556
210.083745	6248.271908	26.386573
210.273101	6273.443434	26.391591
210.622435	6283.405272	26.396608
211.122168	6284.073200	26.401626
210.927632	6300.235882	26.406644
211.270689	6302.517316	26.411661
211.435588	6314.400017	26.416679
211.606506	6334.356599	26.421696
212.073034	6333.764664	26.426714
212.123734	6339.390151	26.431732
212.094339	6349.709029	26.436749
212.571882	6364.359430	26.441767
212.645920	6364.095214	26.446784
212.839076	6370.008785	26.451802
213.086546	6390.640895	26.456820
213.237749	6395.035571	26.461837
213.288636	6406.517948	26.466855
213.380092	6419.159896	26.471872
213.676789	6425.380356	26.476890
214.204882	6448.182640	26.481908
214.144723	6446.168736	26.486925
214.247323	6456.664133	26.491943
214.830969	6481.261738	26.496960
214.874177	6482.274688	26.501978
214.891779	6496.295144	26.506996
215.336933	6510.914662	26.512013
215.795797	6514.587613	26.517031
215.552074	6530.354758	26.522048
216.291501	6533.837430	26.527066
216.372281	6543.009819	26.532084
216.494749	6550.422574	26.537101
216.721809	6561.465488	26.542119
217.227280	6571.895955	26.547136
217.369175	6569.524088	26.552154
217.679317	6594.685560	26.557172
218.037747	6592.123382	26.562189
218.093679	6595.963659	26.567207
218.113367	6599.458014	26.572224
218.505343	6608.701216	26.577242
218.963582	6621.933981	26.582260
218.697144	6624.214278	26.587277
219.258831	6635.447026	26.592295
219.089652	6643.874093	26.597312
219.678364	6642.407411	26.602330
219.379089	6658.824796	26.607348
219.620066	6670.893931	26.612365
220.066153	6679.211920	26.617383
219.888364	6684.716600	26.622400
220.388961	6698.867969	26.627418
220.605475	6711.162131	26.632436
220.658951	6731.007359	26.637453
220.864160	6744.466258	26.642471
221.042201	6745.053310	26.647488
221.073206	6769.471191	26.652506
221.392452	6782.081070	26.657524
221.945455	6794.208359	26.662541
222.434991	6796.883532	26.667559
222.586469	6820.527737	26.672576
223.172243	6827.221583	26.677594
223.122577	6835.092310	26.682612
223.217283	6826.857482	26.687629
223.405995	6838.298551	26.692647
223.737116	6851.348001	26.697664
224.263043	6851.704140	26.702682
223.792130	6859.205347	26.707700
224.034515	6874.066843	26.712717
224.641564	6878.010535	26.717735
224.664767	6883.548554	26.722752
225.046345	6879.102139	26.727770
225.331636	6891.592421	26.732788
225.907271	6901.385629	26.737805
225.885527	6903.792980	26.742823
225.818642	6908.277653	26.747840
226.128213	6909.773766	26.752858
226.180413	6920.503344	26.757876
226.493612	6920.188404	26.762893
226.636545	6916.258409	26.767911
226.304467	6933.227378	26.772928
226.780761	6943.709971	26.777946
227.347009	6951.768979	26.782964
227.351815	6975.357343	26.787981
227.754977	6978.748955	26.792999
227.476689	6997.727628	26.798016
227.868544	7001.057314	26.803034
228.159421	7019.832768	26.808052
228.313199	7038.773303	26.813069
228.515404	7045.750281	26.818087
228.779257	7067.398879	26.823104
229.009082	7075.513945	26.828122
229.366724	7087.701731	26.833140
229.520854	7108.570034	26.838157
230.254438	7109.971825	26.843175
229.920102	7136.489590	26.848192
230.764933	7137.601406	26.853210
230.742680	7142.008219	26.858228
230.896316	7161.170033	26.863245
231.444667	7163.211941	26.868263
231.404642	7171.209562	26.873280
231.607393	7187.191849	26.878298
231.775151	7200.924657	26.883316
231.998480	7196.781917	26.888333
232.419797	7224.272296	26.893351
232.423527	7229.841086	26.898368
232.583755	7240.246807	26.903386
232.911135	7260.226904	26.908404
233.258632	7263.240331	26.913421
233.640231	7264.939808	26.918439
233.774594	7283.831820	26.923456
234.154383	7285.821932	26.928474
234.154650	7301.549423	26.933492
234.379643	7319.455676	26.938509
234.480193	7319.573557	26.943527
234.743846	7337.859616	26.948544
235.530371	7342.612816	26.953562
235.499876	7355.821859	26.958580
235.729535	7365.434476	26.963597
236.040964	7373.977331	26.968615
236.020315	7379.636617	26.973632
236.319183	7381.418539	26.978650
236.712782	7396.885145	26.983668
236.825117	7398.800667	26.988685
236.900933	7404.461109	26.993703
237.089124	7424.093010	26.998720
237.563760	7426.093989	27.003738
237.319771	7429.922492	27.008756
237.973522	7446.721518	27.013773
238.064267	7455.557685	27.018791
238.213698	7458.995365	27.023808
238.515325	7475.029869	27.028826
238.873590	7487.543643	27.033844
238.722020	7490.132301	27.038861
239.201053	7502.676408	27.043879
238.858566	7509.575194	27.048896
239.492164	7521.302317	27.053914
239.767839	7536.128483	27.058932
240.231558	7552.228508	27.063949
240.726454	7562.854932	27.068967
240.940969	7575.774894	27.073984
240.857477	7571.017641	27.079002
241.156168	7586.597144	27.084020
241.303997	7598.609494	27.089037
241.643473	7607.667339	27.094055
241.876632	7626.733670	27.099072
241.978726	7623.290772	27.104090
242.716304	7645.771161	27.109108
242.708383	7656.710715	27.114125
242.665219	7662.090428	27.119143
243.002834	7681.343188	27.124160
243.212094	7685.034195	27.129178
243.651784	7708.082280	27.134196
243.953460	7719.147999	27.139213
244.098123	7717.537981	27.144231
244.235603	7742.780071	27.149248
244.643641	7749.918927	27.154266
244.805306	7761.856024	27.159284
244.969564	7769.864680	27.164301
245.212553	7782.644155	27.169319
245.245680	7792.805349	27.174336
245.805443	7807.128545	27.179354
246.178859	7818.827348	27.184372
246.398510	7846.089785	27.189389
246.827878	7841.801502	27.194407
246.617601	7849.800658	27.199424
247.029666	7855.761765	27.204442
247.333839	7864.285602	27.209460
247.134777	7881.084148	27.214477
248.014103	7891.517335	27.219495
247.766034	7905.183311	27.224512
248.180947	7919.118169	27.229530
248.477109	7923.815174	27.234548
248.795443	7935.455966	27.239565
249.395158	7943.317401	27.244583
249.233950	7956.805121	27.249600
249.489134	7965.861672	27.254618
249.853241	7980.625399	27.259636
249.980957	7982.592054	27.264653
250.116608	7997.103430	27.269671
250.440860	8002.239782	27.274688
250.707671	8019.478054	27.279706
250.895467	8023.772170	27.284724
250.945443	8035.431424	27.289741
251.113842	8043.318388	27.294759
251.350465	8059.620409	27.299776
251.750161	8061.007066	27.304794
251.936835	8085.428259	27.309812
251.796404	8106.740717	27.314829
252.538722	8111.070795	27.319847
252.951926	8125.161136	27.324864
253.252870	8129.999870	27.329882
253.381394	8143.031606	27.334900
253.084933	8158.756545	27.339917
253.788226	8164.490765	27.344935
254.002878	8187.063987	27.349952
254.459981	8192.384213	27.354970
254.868473	8200.112595	27.359988
255.080762	8215.213938	27.365005
255.502627	8216.195763	27.370023
255.424936	8230.886949	27.375040
255.692466	8245.823320	27.380058
255.892567	8257.282553	27.385076
256.100951	8272.160312	27.390093
256.295435	8281.073680	27.395111
256.296891	8296.231532	27.400128
256.668339	8310.959008	27.405146
256.964367	8323.258750	27.410164
257.159282	8336.435091	27.415181
257.469098	8356.099588	27.420199
258.018906	8363.477000	27.425216
258.323394	8370.333249	27.430234
258.495553	8387.281718	27.435252
258.459256	8403.132658	27.440269
258.848260	8414.609116	27.445287
259.017514	8422.446963	27.450304
259.189054	8453.846656	27.455322
259.782401	8454.231841	27.460340
259.613507	8484.261568	27.465357
260.358635	8495.456268	27.470375
260.404625	8519.303727	27.475392
260.982717	8525.613209	27.480410
260.943415	8539.872862	27.485428
261.390956	8549.891398	27.490445
261.866120	8551.228304	27.495463
262.248355	8572.976686	27.500480
262.171494	8575.349811	27.505498
262.740818	8577.755284	27.510516
263.014213	8598.572434	27.515533
263.051493	8593.849506	27.520551
263.186074	8611.233085	27.525568
263.900044	8624.214810	27.530586
263.836737	8626.934384	27.535604
264.120034	8637.664560	27.540621
264.478492	8651.222338	27.545639
264.656763	8663.837405	27.550656
264.513639	8669.554473	27.555674
264.841535	8676.594811	27.560692
265.066876	8691.601700	27.565709
265.346633	8694.186338	27.570727
265.622377	8708.994384	27.575744
265.957774	8723.103204	27.580762
266.135345	8731.866876	27.585780
266.231757	8755.488699	27.590797
266.659144	8761.672791	27.595815
266.922366	8774.572259	27.600832
266.732966	8792.661620	27.605850
267.194266	8802.746990	27.610868
267.550921	8817.822784	27.615885
267.922242	8846.306209	27.620903
267.670762	8858.940758	27.625920
268.524639	8870.062144	27.630938
268.621147	8887.398602	27.635956
268.793221	8908.183544	27.640973
268.987339	8912.766106	27.645991
269.686092	8939.024812	27.651008
269.688996	8960.589881	27.656026
270.308136	8967.424582	27.661044
270.250977	8984.167512	27.666061
270.825001	8993.021204	27.671079
271.283819	8997.062293	27.676096
271.579135	9025.235532	27.681114
272.049694	9031.149233	27.686132
271.955720	9038.555627	27.691149
271.853765	9051.912124	27.696167
272.223845	9063.866228	27.701184
272.320648	9093.047034	27.706202
273.145113	9098.405828	27.711220
273.163679	9118.356982	27.716237
273.499481	9133.109840	27.721255
273.528496	9148.284621	27.726272
273.917930	9160.408845	27.731290
274.453298	9172.570805	27.736308
274.492587	9193.066072	27.741325
274.888006	9198.583788	27.746343
275.497702	9212.392807	27.751360
275.431603	9225.477363	27.756378
275.704595	9238.346164	27.761396
276.232385	9249.713796	27.766413
276.167672	9258.241358	27.771431
276.463865	9278.960208	27.776448
276.802651	9291.663147	27.781466
277.206753	9296.322138	27.786484
277.008631	9310.401657	27.791501
277.565364	9324.613089	27.796519
277.720534	9335.398029	27.801536
277.912449	9356.856027	27.806554
278.288300	9371.151421	27.811572
278.388586	9398.748135	27.816589
278.507125	9398.690040	27.821607
278.511082	9417.433588	27.826624
279.022831	9437.151133	27.831642
279.582089	9452.464808	27.836660
279.702859	9472.373386	27.841677
280.148230	9491.921765	27.846695
280.599041	9503.229460	27.851712
280.891692	9519.503684	27.856730
281.156946	9518.312593	27.861748
281.710645	9534.690026	27.866765
281.712549	9550.400732	27.871783
282.103194	9552.126588	27.876800
282.056793	9572.220909	27.881818
282.543737	9579.169041	27.886836
282.594404	9599.631177	27.891853
282.921864	9618.461919	27.896871
283.466150	9623.311936	27.901888
283.573454	9641.510845	27.906906
284.254996	9649.736322	27.911924
284.327974	9667.113632	27.916941
284.494379	9683.005624	27.921959
284.756401	9694.093692	27.926976
284.928888	9705.687109	27.931994
285.424859	9714.946372	27.937012
285.583423	9739.035167	27.942029
285.775429	9756.686755	27.947047
286.381297	9755.486607	27.952064
286.506274	9771.488782	27.957082
287.216656	9779.045531	27.962100
287.484529	9788.650083	27.967117
287.599852	9779.961380	27.972135
288.192496	9797.582608	27.977152
288.361955	9806.397390	27.982170
288.915774	9802.981154	27.987188
288.889127	9821.403883	27.992205
289.150573	9832.149813	27.997223
289.998334	9833.093388	28.002240
289.688311	9844.667806	28.007258
290.011808	9854.785693	28.012276
290.471197	9874.038797	28.017293
290.562200	9864.110105	28.022311
290.663483	9887.756544	28.027328
290.778357	9908.013697	28.032346
290.879767	9913.036707	28.037364
291.214910	9930.087650	28.042381
291.256391	9958.331432	28.047399
291.902738	9972.022778	28.052416
291.951640	9992.708447	28.057434
292.370682	10004.291915	28.062452
292.552170	10028.067055	28.067469
292.750163	10045.265906	28.072487
293.157138	10060.391599	28.077504
293.617889	10086.199966	28.082522
293.751904	10097.120252	28.087540
294.060685	10111.118152	28.092557
294.467853	10132.103417	28.097575
295.057444	10153.169422	28.102592
295.204711	10161.215517	28.107610
295.314733	10175.315199	28.112628
295.436154	10191.802388	28.117645
295.860317	10201.789171	28.122663
296.332135	10215.760003	28.127680
296.049053	10239.330531	28.132698
296.965150	10251.082086	28.137716
297.279129	10259.674204	28.142733
297.440518	10284.421352	28.147751
297.618682	10281.295871	28.152768
297.839799	10299.106366	28.157786
298.546388	10308.818010	28.162804
299.151245	10309.239992	28.167821
299.375144	10321.610330	28.172839
300.059475	10329.423749	28.177856
299.940183	10333.380274	28.182874
300.248618	10344.240281	28.187892
300.645452	10358.792594	28.192909
300.372576	10370.573589	28.197927
301.204580	10379.527476	28.202944
301.370772	10393.318561	28.207962
301.575650	10411.166406	28.212980
301.739844	10429.215147	28.217997
301.816189	10437.820451	28.223015
302.111021	10445.948246	28.228032
302.234355	10471.835845	28.233050
302.690926	10478.222595	28.238068
303.171791	10490.811042	28.243085
303.327162	10517.316138	28.248103
303.840730	10527.055934	28.253120
303.889280	10545.826047	28.258138
304.077112	10564.931289	28.263156
304.613769	10579.017262	28.268173
304.911166	10601.701151	28.273191
305.582805	10604.211471	28.278208
305.517141	10641.194134	28.283226
305.702961	10641.230381	28.288244
306.224457	10657.406801	28.293261
306.478458	10677.029334	28.298279
306.938500	10694.154895	28.303296
307.111495	10713.627080	28.308314
307.510102	10724.297092	28.313332
308.093994	10727.053197	28.318349
308.336012	10745.176092	28.323367
308.721204	10739.309377	28.328384
308.731840	10760.227680	28.333402
309.059638	10779.876757	28.338420
309.502779	10793.129818	28.343437
309.421405	10803.528126	28.348455
309.670687	10819.249918	28.353472
310.058622	10842.415371	28.358490
310.199033	10862.105438	28.363508
311.068785	10880.324420	28.368525
311.156898	10893.230013	28.373543
311.372933	10900.343145	28.378560
311.316520	10924.534605	28.383578
312.157387	10938.600766	28.388596
312.155527	10945.270524	28.393613
312.316146	10971.215214	28.398631
312.931647	10974.041491	28.403648
313.146094	10982.336647	28.408666
313.382383	11001.780229	28.413684
313.563139	11026.712824	28.418701
314.116414	11039.030865	28.423719
314.189601	11057.348288	28.428736
314.313247	11079.097057	28.433754
314.407811	11104.352824	28.438772
315.081104	11120.408745	28.443789
314.962413	11143.097784	28.448807
315.901448	11170.687636	28.453824
316.156724	11193.326201	28.458842
316.552857	11207.787758	28.463860
317.069046	11228.385301	28.468877
317.372679	11247.811776	28.473895
317.463878	11252.361091	28.478912
317.678307	11270.526793	28.483930
318.079894	11287.792998	28.488948
318.412908	11303.265049	28.493965
318.629542	11324.237090	28.498983
318.942554	11344.206442	28.504000
319.353449	11364.583262	28.509018
320.009324	11377.571541	28.514036
320.398434	11401.463725	28.519053
320.548742	11425.841447	28.524071
320.972264	11419.718080	28.529088
321.244586	11446.041673	28.534106
321.215553	11448.408804	28.539124
321.817691	11474.004585	28.544141
321.801679	11493.513999	28.549159
322.343794	11506.817636	28.554176
322.744449	11529.207058	28.559194
323.219106	11541.484718	28.564212
323.428454	11569.821443	28.569229
323.502027	11581.419478	28.574247
324.174673	11591.151932	28.579264
324.388442	11620.169057	28.584282
324.571399	11635.645884	28.589300
325.197127	11641.500681	28.594317
325.442252	11663.570550	28.599335
325.961892	11677.765343	28.604352
326.446024	11695.370681	28.609370
326.220467	11700.518021	28.614388
326.457064	11725.678205	28.619405
326.622432	11738.312866	28.624423
327.464994	11753.649471	28.629440
327.640017	11777.466966	28.634458
327.814387	11794.899831	28.639476
328.264628	11809.785057	28.644493
328.220458	11828.939105	28.649511
328.703763	11840.435833	28.654528
328.939690	11850.640254	28.659546
329.369399	11875.746299	28.664564
329.862648	11894.307311	28.669581
329.902818	11911.043682	28.674599
330.333459	11918.763781	28.679616
330.832187	11933.945019	28.684634
330.981574	11949.905278	28.689652
331.196615	11965.950328	28.694669
331.463733	11989.131287	28.699687
331.712372	12013.270162	28.704704
332.232650	12037.599156	28.709722
332.743762	12052.466066	28.714740
333.274364	12062.387936	28.719757
333.067562	12085.808679	28.724775
333.704857	12104.930032	28.729792
333.913648	12126.764927	28.734810
334.118117	12144.086550	28.739828
334.394365	12158.360333	28.744845
334.908439	12184.730509	28.749863
335.193443	12196.804178	28.754880
335.364568	12229.003238	28.759898
335.730779	12254.475209	28.764916
336.218657	12273.836255	28.769933
336.551053	12289.087649	28.774951
337.124486	12305.432304	28.779968
337.301091	12315.810802	28.784986
337.685961	12342.520818	28.790004
338.204680	12355.728581	28.795021
338.560576	12374.717236	28.800039
338.717721	12394.917071	28.805056
338.903405	12413.669613	28.810074
339.228601	12433.693954	28.815092
340.146515	12455.451142	28.820109
340.094401	12481.720405	28.825127
340.626252	12495.943344	28.830144
340.861208	12506.424641	28.835162
341.029325	12534.588901	28.840180
341.322293	12551.825062	28.845197
341.654893	12572.933250	28.850215
342.121896	12599.373833	28.855232
342.288939	12615.647810	28.860250
342.787385	12639.931468	28.865268
343.604742	12653.055298	28.870285
343.675223	12674.273092	28.875303
344.267488	12686.717132	28.880320
344.734318	12696.225719	28.885338
344.592968	12715.103559	28.890356
345.330764	12720.946239	28.895373
345.346465	12736.658843	28.900391
345.982300	12756.856864	28.905408
346.137184	12775.580128	28.910426
346.364071	12787.238481	28.915444
347.014866	12798.299747	28.920461
347.088115	12821.472534	28.925479
347.352535	12819.291122	28.930496
347.753807	12838.406546	28.935514
347.719029	12856.844889	28.940532
348.045792	12876.990392	28.945549
348.070456	12893.873377	28.950567
348.633239	12905.535556	28.955584
348.839251	12950.057904	28.960602
349.096210	12970.249878	28.965620
349.775276	12981.523237	28.970637
350.000557	13007.919420	28.975655
350.580347	13024.557051	28.980672
350.979368	13050.788462	28.985690
351.088905	13079.220462	28.990708
351.432759	13093.152573	28.995725
351.730858	13121.090383	29.000743
352.298696	13142.328259	29.005760
352.669829	13161.647845	29.010778
352.473247	13187.980410	29.015796
353.275698	13206.571392	29.020813
353.453031	13239.239858	29.025831
353.647509	13274.206806	29.030848
354.326015	13283.906567	29.035866
354.797497	13315.925558	29.040884
354.937573	13331.286382	29.045901
355.284116	13357.140485	29.050919
355.979243	13368.716303	29.055936
356.718472	13387.240147	29.060954
356.838033	13412.787216	29.065972
357.564772	13424.425047	29.070989
357.715458	13438.467564	29.076007
358.082285	13456.958937	29.081024
358.402122	13474.114746	29.086042
358.868840	13491.246652	29.091060
359.142968	13497.751343	29.096077
359.408136	13525.207396	29.101095
359.709643	13548.011942	29.106112
360.311712	13564.156408	29.111130
360.081735	13578.370214	29.116148
360.723874	13594.047143	29.121165
360.834816	13622.823927	29.126183
361.481727	13643.570812	29.131200
361.899181	13654.219827	29.136218
361.986106	13681.276146	29.141236
362.183452	13697.165262	29.146253
362.649138	13729.406555	29.151271
362.761873	13744.405032	29.156288
363.662387	13776.800102	29.161306
363.552707	13804.218781	29.166324
364.202376	13813.430114	29.171341
364.752685	13829.346367	29.176359
364.829021	13866.302929	29.181376
365.027825	13884.908384	29.186394
365.315770	13913.528608	29.191412
365.682947	13929.064319	29.196429
366.202374	13964.733127	29.201447
366.709952	13976.555284	29.206464
366.985313	13999.658195	29.211482
367.557384	14017.045684	29.216500
367.970446	14019.625071	29.221517
368.351761	14046.947149	29.226535
368.317847	14071.448112	29.231552
368.981926	14076.075936	29.236570
369.344497	14101.066770	29.241588
369.760952	14124.333657	29.246605
369.803662	14145.851843	29.251623
370.317794	14171.125746	29.256640
370.913731	14181.882974	29.261658
370.680811	14212.823786	29.266676
371.406623	14222.296494	29.271693
371.444765	14248.278104	29.276711
372.004350	14280.924196	29.281728
372.202784	14296.418684	29.286746
372.738150	14330.110682	29.291764
373.167437	14347.476725	29.296781
373.369153	14370.298107	29.301799
374.097624	14388.060410	29.306816
374.229751	14408.121857	29.311834
374.614086	14437.045538	29.316852
375.316081	14455.588430	29.321869
375.683280	14483.430935	29.326887
375.573488	14504.858894	29.331904
376.333674	14532.378199	29.336922
376.705294	14557.215027	29.341940
377.321769	14579.934910	29.346957
377.434789	14600.669676	29.351975
377.654380	14617.321779	29.356992
378.329693	14635.741219	29.362010
378.618565	14664.233497	29.367028
378.998384	14685.266438	29.372045
379.579594	14708.561788	29.377063
379.503029	14734.972155	29.382080
380.537335	14748.044350	29.387098
380.549527	14777.690922	29.392116
381.043244	14788.468806	29.397133
381.295080	14825.132157	29.402151
381.506044	14845.027906	29.407168
382.127276	14861.803537	29.412186
382.383505	14888.125122	29.417204
382.655661	14903.842976	29.422221
383.212601	14924.587152	29.427239
383.385158	14959.644206	29.432256
383.662468	14973.702891	29.437274
384.215432	14990.641480	29.442292
384.797740	15013.539171	29.447309
385.077223	15043.985522	29.452327
385.274059	15068.082286	29.457344
386.145250	15091.044570	29.462362
386.124013	15118.467150	29.467380
386.832379	15138.519606	29.472397
387.170140	15150.764741	29.477415
387.492686	15174.994565	29.482432
387.659744	15193.800039	29.487450
388.109064	15220.240414	29.492468
388.068706	15236.054264	29.497485
388.637567	15259.678740	29.502503
388.697318	15291.049209	29.507520
389.205841	15310.184302	29.512538
389.419710	15346.603813	29.517556
389.827709	15365.568708	29.522573
390.286663	15392.180352	29.527591
390.827536	15427.483471	29.532608
391.407896	15450.919238	29.537626
391.302679	15469.086762	29.542644
391.966079	15492.140034	29.547661
392.563663	15523.918796	29.552679
392.979869	15545.221878	29.557696
393.775365	15566.129174	29.562714
393.817996	15592.701026	29.567732
394.108327	15627.647054	29.572749
394.700532	15644.227121	29.577767
394.893984	15672.245512	29.582784
395.723807	15692.809967	29.587802
395.948586	15722.554878	29.592820
396.594900	15735.870237	29.597837
396.595719	15764.306831	29.602855
397.065754	15784.006438	29.607872
397.641850	15805.337939	29.612890
397.895451	15833.231702	29.617908
398.138476	15848.865810	29.622925
398.499836	15873.360493	29.627943
399.080023	15908.180669	29.632960
399.359066	15929.505156	29.637978
399.771681	15951.363232	29.642996
400.101753	15967.930505	29.648013
400.706068	15994.490116	29.653031
400.834345	16020.429065	29.658048
401.750959	16039.910029	29.663066
401.895008	16066.550385	29.668084
402.076480	16090.601698	29.673101
402.533044	16118.443168	29.678119
402.879074	16153.885781	29.683136
403.427949	16174.688540	29.688154
403.791716	16198.020511	29.693172
404.198879	16224.471793	29.698189
404.785437	16252.139070	29.703207
404.976397	16286.417274	29.708224
405.452264	16299.786265	29.713242
405.915321	16333.796836	29.718260
406.201584	16357.734242	29.723277
407.001152	16372.596819	29.728295
407.201778	16400.844106	29.733312
407.782596	16422.471743	29.738330
407.782433	16449.939391	29.743348
408.186543	16467.508683	29.748365
408.744861	16488.796335	29.753383
409.062816	16522.528112	29.758400
409.697031	16525.988254	29.763418
409.834926	16557.048289	29.768436
410.059365	16579.969815	29.773453
410.805106	16595.252561	29.778471
411.121761	16614.974131	29.783488
411.358054	16639.616523	29.788506
411.760155	16670.086315	29.793524
412.127937	16693.520553	29.798541
412.439876	16719.162737	29.803559
412.814245	16747.379431	29.808576
413.374150	16771.213058	29.813594
413.425244	16802.196085	29.818612
414.202368	16836.374240	29.823629
414.519363	16865.433687	29.828647
414.711745	16896.351875	29.833664
415.007090	16921.318352	29.838682
415.787128	16959.705832	29.843700
416.010829	16989.912576	29.848717
416.574950	17015.989840	29.853735
416.855338	17046.406150	29.858752
417.552297	17068.013041	29.863770
417.963772	17108.909056	29.868788
418.610134	17127.240056	29.873805
419.186999	17141.406629	29.878823
419.380989	17168.670416	29.883840
419.885362	17196.739863	29.888858
420.147033	17227.235491	29.893876
420.672375	17251.828475	29.898893
421.176722	17271.335359	29.903911
421.253537	17311.322292	29.908928
421.776125	17332.714043	29.913946
422.074763	17362.556443	29.918964
422.405828	17392.470109	29.923981
423.032257	17431.195427	29.928999
423.282559	17462.938550	29.934016
423.621588	17485.708915	29.939034
424.296051	17513.167018	29.944052
424.907181	17540.647466	29.949069
425.661266	17574.170323	29.954087
425.797216	17602.056499	29.959104
426.473101	17622.458119	29.964122
427.275155	17636.207589	29.969140
427.068844	17664.821223	29.974157
427.687399	17684.762782	29.979175
428.312935	17696.591274	29.984192
428.915948	17716.717236	29.989210
429.067255	17752.093558	29.994228
429.345738	17776.829463	29.999245
429.800431	17796.586650	30.004263
430.011741	17821.005382	30.009280
430.205496	17852.342572	30.014298
430.872600	17876.242322	30.019316
431.453539	17899.081838	30.024333
431.794822	17925.850858	30.029351
432.101623	17951.973457	30.034368
432.166130	17971.259575	30.039386
432.778306	18002.133556	30.044404
433.223854	18039.456156	30.049421
433.740308	18055.456218	30.054439
434.155346	18084.886584	30.059456
434.394730	18101.224143	30.064474
434.704863	18122.308319	30.069492
434.970608	18157.751977	30.074509
435.768944	18193.206925	30.079527
435.938482	18220.656576	30.084544
436.441616	18244.553886	30.089562
436.857575	18275.062426	30.094580
437.071465	18322.654605	30.099597
437.772201	18342.398485	30.104615
438.209815	18380.697986	30.109632
438.466747	18411.054568	30.114650
439.033129	18446.161216	30.119668
439.182620	18475.698018	30.124685
440.112740	18510.809854	30.129703
440.531031	18551.336531	30.134720
440.939748	18575.615939	30.139738
441.455298	18607.796322	30.144756
441.904878	18640.287685	30.149773
442.480967	18663.171622	30.154791
442.698165	18693.466186	30.159808
443.290929	18723.075358	30.164826
443.723526	18753.014448	30.169844
443.876986	18788.849102	30.174861
444.483983	18819.044403	30.179879
445.309033	18846.102518	30.184896
445.945278	18865.209279	30.189914
446.305534	18895.279466	30.194932
447.199638	18921.066806	30.199949
447.832903	18918.869104	30.204967
448.591363	18954.583340	30.209984
448.659332	18955.105363	30.215002
449.247441	18978.276449	30.220020
449.855676	18983.261859	30.225037
450.029320	19006.981330	30.230055
450.070480	19030.899906	30.235072
450.596689	19056.829162	30.240090
450.958542	19074.657378	30.245108
450.910506	19104.542609	30.250125
451.892073	19127.038988	30.255143
451.872297	19163.317877	30.260160
452.170818	19194.680453	30.265178
453.078426	19209.912650	30.270196
453.321561	19241.536129	30.275213
453.880170	19262.687392	30.280231
453.928507	19296.648878	30.285248
454.541219	19329.332243	30.290266
455.016494	19361.104822	30.295284
455.265154	19394.206981	30.300301
456.122247	19418.341463	30.305319
456.371585	19456.570448	30.310336
456.538807	19483.882523	30.315354
457.081961	19495.253041	30.320372
457.057460	19526.387012	30.325389
457.914866	19552.527344	30.330407
458.045263	19597.497497	30.335424
458.706546	19627.979056	30.340442
459.057766	19655.802721	30.345460
459.478596	19693.810851	30.350477
460.205803	19720.387998	30.355495
460.533569	19765.298840	30.360512
460.801701	19786.139180	30.365530
461.419339	19812.641410	30.370548
462.110013	19850.295087	30.375565
462.529710	19876.501760	30.380583
463.014089	19917.903842	30.385600
463.592289	19953.729413	30.390618
464.037164	19975.015524	30.395636
464.335357	20005.690722	30.400653
464.918890	20040.828552	30.405671
465.239242	20071.152668	30.410688
465.821269	20112.269202	30.415706
466.198003	20145.761655	30.420724
466.554102	20185.911096	30.425741
467.200849	20202.803367	30.430759
467.997599	20243.432435	30.435776
468.262584	20265.375638	30.440794
469.141672	20300.613444	30.445812
469.229479	20333.848350	30.450829
469.697608	20353.153434	30.455847
470.052400	20390.377602	30.460864
470.752725	20419.633445	30.465882
471.198644	20444.298478	30.470900
471.409657	20486.504781	30.475917
471.782090	20510.542159	30.480935
472.483989	20554.653816	30.485952
472.628555	20589.257598	30.490970
473.599047	20617.715535	30.495988
473.916219	20667.658223	30.501005
474.445048	20688.539742	30.506023
475.176993	20726.526412	30.511040
475.116577	20759.164467	30.516058
475.876215	20794.574804	30.521076
476.023704	20830.909656	30.526093
477.072769	20859.716997	30.531111
477.639182	20887.660958	30.536128
477.943051	20914.707257	30.541146
478.455985	20943.700969	30.546164
478.577278	20981.584714	30.551181
479.509400	21004.258651	30.556199
479.555394	21034.407430	30.561216
480.056726	21071.145608	30.566234
480.609230	21102.955100	30.571252
480.860807	21145.255548	30.576269
481.580987	21171.590962	30.581287
482.146238	21207.478956	30.586304
482.390940	21235.588983	30.591322
483.100745	21251.814735	30.596340
483.040846	21288.589274	30.601357
483.870911	21324.426686	30.606375
484.506362	21353.644206	30.611392
484.728113	21380.848513	30.616410
485.093694	21410.406042	30.621428
485.433337	21447.270091	30.626445
486.032610	21475.938366	30.631463
486.439012	21508.874552	30.636480
486.880369	21540.538034	30.641498
487.262806	21574.101145	30.646516
487.647033	21612.337520	30.651533
488.216855	21656.110240	30.656551
488.912059	21694.508347	30.661568
489.417084	21738.015176	30.666586
490.231714	21777.612064	30.671604
490.421687	21817.290446	30.676621
490.997486	21842.181138	30.681639
491.867631	21877.673189	30.686656
491.838480	21915.850926	30.691674
492.488971	21953.110840	30.696692
492.693970	21992.180821	30.701709
493.123861	22022.789358	30.706727
493.460937	22068.499984	30.711744
494.296376	22097.530296	30.716762
495.157190	22141.042206	30.721780
495.383923	22184.111009	30.726797
495.751960	22208.765229	30.731815
496.728806	22245.094090	30.736832
496.940962	22291.793232	30.741850
497.874531	22314.939831	30.746868
498.258122	22355.422014	30.751885
498.868985	22383.853814	30.756903
499.467517	22422.356520	30.761920
499.771099	22456.075052	30.766938
500.064260	22485.891871	30.771956
500.688454	22519.983994	30.776973
501.360728	22552.615366	30.781991
501.616844	22585.643902	30.787008
502.001500	22635.608065	30.792026
502.862438	22651.934852	30.797044
503.017324	22691.884873	30.802061
503.399065	22732.732989	30.807079
504.148440	22756.877581	30.812096
504.515552	22802.665096	30.817114
505.024060	22834.837168	30.822132
505.227387	22881.398468	30.827149
505.770836	22918.482379	30.832167
506.558842	22962.887949	30.837184
506.797276	22999.338537	30.842202
507.728019	23031.802128	30.847220
508.074057	23076.304412	30.852237
508.387107	23112.941863	30.857255
508.945883	23136.670013	30.862272
509.382024	23177.590163	30.867290
510.210140	23205.566653	30.872308
510.290069	23238.481261	30.877325
511.129373	23269.209732	30.882343
511.741670	23300.485615	30.887360
511.628521	23336.692097	30.892378
512.441643	23375.101503	30.897396
513.321800	23410.419762	30.902413
513.397731	23450.626083	30.907431
513.850502	23489.758747	30.912448
514.455816	23521.789979	30.917466
515.218001	23554.933688	30.922484
515.640239	23604.642862	30.927501
516.185340	23624.522189	30.932519
516.630113	23662.248187	30.937536
517.195101	23702.470976	30.942554
517.703465	23734.940279	30.947572
518.436001	23762.569072	30.952589
518.684792	23806.751765	30.957607
519.157860	23834.856029	30.962624
519.880629	23872.372042	30.967642
520.786628	23908.005522	30.972660
520.867887	23949.995587	30.977677
521.389583	23974.597361	30.982695
521.861109	24016.131588	30.987712
522.181265	24059.290638	30.992730
523.114075	24094.947836	30.997748
523.701137	24144.853000	31.002765
523.892822	24177.099530	31.007783
524.293000	24215.964300	31.012800
525.095321	24254.860421	31.017818
526.044523	24284.179116	31.022836
526.237006	24317.682987	31.027853
526.953819	24349.514594	31.032871
527.859352	24389.623437	31.037888
528.028356	24419.314786	31.042906
528.641067	24458.707149	31.047924
528.685645	24488.578354	31.052941
529.332582	24525.358080	31.057959
529.685574	24560.651016	31.062976
530.260719	24605.269964	31.067994
530.827966	24645.856345	31.073012
531.275288	24690.880303	31.078029
531.432621	24735.800911	31.083047
532.227464	24767.631166	31.088064
532.540931	24823.428589	31.093082
533.340055	24857.400195	31.098100
534.156408	24898.513924	31.103117
534.559132	24942.189208	31.108135
535.302211	24976.152665	31.113152
535.254608	25020.126761	31.118170
536.240698	25050.300426	31.123188
536.766349	25098.553848	31.128205
537.265001	25133.548349	31.133223
537.718980	25167.292790	31.138240
537.960849	25204.790075	31.143258
538.596043	25242.200377	31.148276
538.944987	25279.974617	31.153293
540.013502	25313.343403	31.158311
540.780893	25343.758065	31.163328
541.376438	25373.551828	31.168346
542.083551	25400.512408	31.173364
542.362998	25437.721446	31.178381
542.882987	25466.276445	31.183399
543.437935	25496.036727	31.188416
543.683207	25534.552828	31.193434
544.223021	25562.626664	31.198452
544.681669	25595.489749	31.203469
545.625855	25636.324266	31.208487
545.874828	25679.088598	31.213504
545.925631	25722.933144	31.218522
546.405417	25757.021342	31.223540
546.806433	25807.040113	31.228557
547.350140	25855.090480	31.233575
548.121906	25899.876308	31.238592
548.490230	25951.421168	31.243610
549.015339	26005.500763	31.248628
550.124416	26040.332271	31.253645
550.686591	26078.892162	31.258663
551.574311	26115.469400	31.263680
552.114804	26152.416358	31.268698
552.589238	26195.880387	31.273716
552.795357	26227.261378	31.278733
553.148134	26277.758043	31.283751
554.067333	26315.917368	31.288768
554.595186	26362.181877	31.293786
555.487454	26407.916578	31.298804
555.900042	26451.529016	31.303821
556.440925	26486.682039	31.308839
557.285044	26521.662365	31.313856
557.735427	26573.278871	31.318874
558.402629	26594.358858	31.323892
558.814102	26633.519984	31.328909
558.714120	26670.659958	31.333927
559.895901	26701.355482	31.338944
560.329594	26756.110788	31.343962
560.824671	26780.659678	31.348980
562.054339	26821.330423	31.353997
562.474301	26857.498551	31.359015
563.058817	26884.457525	31.364032
563.628651	26920.121343	31.369050
564.589269	26953.513895	31.374068
564.678417	26993.457562	31.379085
565.297271	27027.509765	31.384103
566.178943	27057.398962	31.389120
566.392624	27092.133504	31.394138
566.658327	27128.088092	31.399156
567.635874	27158.029962	31.404173
568.094563	27198.350172	31.409191
568.492798	27219.445458	31.414208
568.716843	27254.491476	31.419226
569.190982	27281.261490	31.424244
569.897327	27308.390070	31.429261
570.222644	27348.850077	31.434279
571.028690	27382.547832	31.439296
571.726954	27410.853360	31.444314
572.242237	27447.955431	31.449332
572.564060	27486.330076	31.454349
572.909160	27538.696795	31.459367
573.815017	27568.964422	31.464384
574.171189	27620.570136	31.469402
574.370986	27654.196410	31.474420
575.135932	27703.411481	31.479437
575.510209	27753.451588	31.484455
576.465527	27792.548612	31.489472
576.781785	27834.446797	31.494490
577.492346	27881.113603	31.499508
577.907410	27926.013890	31.504525
578.442651	27971.092133	31.509543
579.229551	28014.174875	31.514560
579.670967	28077.038474	31.519578
580.349576	28108.104414	31.524596
581.310091	28152.929490	31.529613
581.763584	28213.516246	31.534631
582.297496	28253.244062	31.539648
582.763690	28294.593239	31.544666
583.234066	28350.543360	31.549684
583.853019	28389.512606	31.554701
584.381546	28433.718627	31.559719
585.287362	28471.564521	31.564736
585.840544	28527.686437	31.569754
586.471024	28568.915600	31.574772
587.151415	28610.883868	31.579789
587.911299	28660.498194	31.584807
588.401338	28697.772617	31.589824
589.249386	28748.060240	31.594842
589.715521	28783.381456	31.599860
590.369012	28834.111631	31.604877
590.784891	28865.529738	31.609895
591.664342	28897.821175	31.614912
592.032232	28947.763555	31.619930
592.396537	28989.592463	31.624948
593.477887	29018.977587	31.629965
593.589402	29068.176378	31.634983
594.068395	29109.905384	31.640000
594.792704	29160.524444	31.645018
595.387897	29207.252843	31.650036
596.196472	29249.679847	31.655053
596.460330	29302.077805	31.660071
597.406036	29343.662168	31.665088
597.835622	29393.761563	31.670106
598.115424	29431.862263	31.675124
598.785969	29482.686302	31.680141
599.146756	29538.498798	31.685159
599.824378	29568.756094	31.690176
600.673018	29613.338273	31.695194
600.803467	29654.802693	31.700212
601.588640	29701.946672	31.705229
601.968968	29741.713623	31.710247
602.679600	29789.723893	31.715264
603.121925	29841.489996	31.720282
603.701863	29890.452769	31.725300
604.372684	29929.819323	31.730317
604.870675	29994.561458	31.735335
605.163332	30042.771419	31.740352
606.051834	30103.381040	31.745370
606.394023	30156.612419	31.750388
607.340938	30201.405924	31.755405
607.486057	30272.389559	31.760423
608.556496	30309.879414	31.765440
609.146785	30372.761269	31.770458
609.666650	30425.330095	31.775476
610.629523	30476.778910	31.780493
610.999934	30535.310340	31.785511
611.659621	30584.216789	31.790528
612.414452	30644.179890	31.795546
613.132642	30690.683340	31.800564
613.909844	30737.707076	31.805581
614.511616	30793.085164	31.810599
615.056758	30835.723737	31.815616
615.781111	30887.695680	31.820634
616.070189	30936.443129	31.825652
617.162041	30983.482083	31.830669
617.732217	31028.859534	31.835687
618.443244	31082.567900	31.840704
619.026607	31131.379389	31.845722
619.779172	31173.903855	31.850740
620.383429	31219.400918	31.855757
620.793693	31273.030141	31.860775
621.271754	31311.404682	31.865792
621.660486	31363.171524	31.870810
622.294476	31419.068287	31.875828
623.303524	31464.763204	31.880845
623.809360	31515.273050	31.885863
624.932930	31559.939702	31.890880
625.329058	31611.603701	31.895898
625.845236	31661.240749	31.900916
626.634927	31710.405681	31.905933
626.891273	31763.205170	31.910951
627.782830	31809.567554	31.915968
628.297161	31854.628344	31.920986
628.903380	31912.000182	31.926004
629.942046	31951.090787	31.931021
630.275940	32003.443677	31.936039
630.706765	32046.915328	31.941056
631.166569	32103.155815	31.946074
631.995188	32141.437067	31.951092
632.658575	32194.764189	31.956109
633.319110	32247.488257	31.961127
634.034544	32290.960941	31.966144
634.169534	32340.389633	31.971162
635.020988	32381.065207	31.976180
635.911008	32426.148123	31.981197
636.561568	32459.517060	31.986215
636.891107	32512.335665	31.991232
637.535701	32560.911522	31.996250
638.169724	32604.563501	32.001268
638.775154	32642.260428	32.006285
639.029833	32696.395084	32.011303
640.084900	32739.099258	32.016320
641.029776	32788.602084	32.021338
641.201722	32855.976693	32.026356
642.314506	32898.738294	32.031373
643.074718	32938.512396	32.036391
643.483458	32992.106476	32.041408
644.028125	33035.658758	32.046426
644.638426	33086.963836	32.051444
645.193617	33142.918406	32.056461
645.795078	33194.073901	32.061479
646.437301	33251.241325	32.066496
647.488505	33291.267860	32.071514
647.721026	33348.201363	32.076532
648.289062	33390.874439	32.081549
648.912001	33447.708284	32.086567
649.565977	33504.343496	32.091584
650.425123	33550.771115	32.096602
650.949132	33614.582295	32.101620
651.766641	33660.036379	32.106637
652.087738	33728.177369	32.111655
652.850917	33786.958885	32.116672
653.525644	33834.364044	32.121690
653.792143	33901.445679	32.126708
654.551269	33960.223726	32.131725
655.508957	34016.356759	32.136743
656.230529	34072.902756	32.141760
657.063261	34129.848982	32.146778
657.531274	34189.823371	32.151796
658.560423	34232.601745	32.156813
658.970786	34298.602747	32.161831
659.743969	34344.756225	32.166848
660.641673	34398.182406	32.171866
660.992059	34447.860528	32.176884
661.657481	34498.341470	32.181901
662.427693	34551.487351	32.186919
663.464476	34601.242653	32.191936
664.063262	34650.426243	32.196954
664.078234	34701.842146	32.201972
665.106164	34746.548431	32.206989
665.575057	34816.327170	32.212007
666.594327	34870.476438	32.217024
667.326923	34919.045198	32.222042
667.389038	34984.065490	32.227060
668.398106	35038.905839	32.232077
668.864455	35081.750793	32.237095
669.859100	35125.188040	32.242112
670.461804	35182.038922	32.247130
670.887547	35219.871219	32.252148
671.987354	35262.975212	32.257165
672.054711	35317.594375	32.262183
672.595857	35371.603849	32.267200
673.226136	35415.039963	32.272218
673.648401	35475.410926	32.277236
674.642329	35524.921998	32.282253
675.225482	35584.317107	32.287271
675.670984	35650.161788	32.292288
676.528815	35703.786113	32.297306
677.064878	35765.527340	32.302324
678.016307	35812.920880	32.307341
678.636687	35871.396694	32.312359
679.528508	35930.244123	32.317376
680.290996	35985.401165	32.322394
680.653781	36053.357406	32.327412
681.368396	36104.645725	32.332429
681.884335	36159.937191	32.337447
682.847047	36216.171436	32.342464
683.507513	36289.130978	32.347482
684.075146	36346.224735	32.352500
684.975478	36397.167487	32.357517
685.347502	36461.005872	32.362535
685.829490	36529.555202	32.367552
686.889363	36584.063029	32.372570
687.436734	36653.392331	32.377588
688.222856	36715.953342	32.382605
688.867473	36792.018792	32.387623
689.911771	36846.744374	32.392640
690.761335	36899.486206	32.397658
691.387007	36963.601441	32.402676
692.459502	37005.218053	32.407693
693.069665	37060.797046	32.412711
693.398847	37119.329880	32.417728
694.235594	37166.874798	32.422746
694.682512	37224.520516	32.427764
695.266160	37291.940491	32.432781
696.123527	37346.473578	32.437799
696.931692	37408.385644	32.442816
697.638655	37467.097616	32.447834
698.207926	37539.066448	32.452852
699.004891	37588.386362	32.457869
699.495360	37655.879389	32.462887
700.062928	37715.033821	32.467904
701.178503	37769.765252	32.472922
701.684321	37833.740479	32.477940
702.401161	37899.716325	32.482957
702.954163	37960.622524	32.487975
703.879555	38018.179006	32.492992
704.654910	38076.259400	32.498010
705.020892	38148.114980	32.503028
706.183837	38208.185466	32.508045
706.923462	38260.020358	32.513063
707.393480	38306.775433	32.518080
708.434648	38347.988824	32.523098
708.954189	38403.544097	32.528116
709.248557	38457.571241	32.533133
709.862148	38507.468601	32.538151
710.569895	38578.049589	32.543168
711.054947	38628.552759	32.548186
711.606394	38697.421504	32.553204
712.364580	38752.001730	32.558221
713.463239	38815.271331	32.563239
713.905554	38888.011946	32.568256
714.802338	38936.028492	32.573274
715.690282	38993.750365	32.578292
716.358704	39053.696025	32.583309
717.086311	39115.203003	32.588327
717.558798	39182.933622	32.593344
718.716580	39229.428793	32.598362
719.217413	39296.754834	32.603380
720.044842	39367.310591	32.608397
720.638785	39423.634752	32.613415
721.389543	39495.718617	32.618432
721.643658	39544.824749	32.623450
722.700339	39610.177593	32.628468
723.374321	39677.785068	32.633485
724.088516	39748.579622	32.638503
724.820618	39816.906922	32.643520
725.873925	39881.247397	32.648538
726.257481	39961.717770	32.653556
727.221340	40023.518421	32.658573
727.951141	40080.565857	32.663591
728.499882	40156.119225	32.668608
729.620711	40208.206882	32.673626
730.183783	40275.004915	32.678644
731.062304	40332.991456	32.683661
731.964856	40407.595479	32.688679
732.251928	40471.533467	32.693696
733.431620	40526.959043	32.698714
733.961814	40598.595404	32.703732
734.698085	40661.311398	32.708749
735.336656	40724.106255	32.713767
736.092059	40795.455270	32.718784
736.699904	40846.863283	32.723802
737.721148	40910.001613	32.728820
738.358924	40980.805560	32.733837
739.487019	41041.129751	32.738855
739.719830	41105.930334	32.743872
740.492421	41158.675603	32.748890
741.119943	41241.956537	32.753908
741.913944	41308.516829	32.758925
743.275757	41370.511331	32.763943
743.670027	41434.221368	32.768960
744.486088	41504.374584	32.773978
745.119861	41566.501468	32.778996
745.756615	41628.432546	32.784013
746.607597	41689.471815	32.789031
746.842533	41759.705970	32.794048
748.104501	41804.127192	32.799066
748.838897	41871.046114	32.804084
749.293639	41927.629368	32.809101
750.250726	41987.630848	32.814119
750.629160	42044.542055	32.819136
751.331410	42098.534711	32.824154
752.302106	42165.685272	32.829172
752.794673	42229.720112	32.834189
753.444497	42295.338828	32.839207
754.105819	42366.974313	32.844224
755.020669	42432.450425	32.849242
755.479912	42505.680027	32.854260
756.459842	42584.788700	32.859277
757.672423	42652.388419	32.864295
758.260208	42716.472996	32.869312
758.551498	42787.686521	32.874330
759.197221	42865.733046	32.879348
760.020700	42938.985362	32.884365
760.967555	43001.666919	32.889383
761.899539	43086.892424	32.894400
763.252492	43143.525948	32.899418
764.188265	43207.620041	32.904436
764.672114	43280.003623	32.909453
765.587294	43339.549630	32.914471
766.130870	43395.445351	32.919488
767.024807	43464.994811	32.924506
767.666427	43524.660710	32.929524
768.055391	43603.934370	32.934541
768.838979	43669.887166	32.939559
769.695583	43757.181559	32.944576
770.378488	43811.050165	32.949594
771.344146	43888.529876	32.954612
771.955741	43959.189349	32.959629
773.884662	44018.995881	32.964647
774.715003	44077.684117	32.969664
775.466788	44140.085396	32.974682
775.841783	44196.161956	32.979700
776.674510	44261.740094	32.984717
777.602413	44314.476614	32.989735
777.763989	44386.808858	32.994752
778.676017	44452.510743	32.999770
779.549265	44518.392556	33.004788
779.978120	44583.540916	33.009805
781.188352	44644.561842	33.014823
781.978632	44720.237157	33.019840
782.544389	44782.105663	33.024858
783.403976	44855.776758	33.029876
783.834540	44916.506323	33.034893
784.665534	44988.491593	33.039911
785.469274	45070.327511	33.044928
786.532883	45134.641833	33.049946
787.306490	45218.978673	33.054964
787.827118	45291.289064	33.059981
788.774721	45337.741186	33.064999
789.607220	45397.629209	33.070016
790.190043	45453.430658	33.075034
791.059992	45525.052292	33.080052
791.757237	45593.146186	33.085069
792.688300	45654.833445	33.090087
792.814922	45727.738376	33.095104
793.863466	45784.135586	33.100122
794.697708	45853.770360	33.105140
795.119139	45924.083174	33.110157
796.014375	45991.983050	33.115175
796.463647	46074.397503	33.120192
797.399522	46143.036063	33.125210
798.255341	46226.891437	33.130228
798.993543	46299.606749	33.135245
799.822091	46377.305499	33.140263
800.725466	46461.299554	33.145280
801.698410	46534.887121	33.150298
802.902846	46600.074142	33.155316
803.255491	46675.344862	33.160333
804.205468	46744.283263	33.165351
805.103044	46822.925829	33.170368
805.911138	46901.453632	33.175386
806.557538	46982.563158	33.180404
807.188924	47053.733663	33.185421
808.299606	47122.881450	33.190439
808.806955	47220.386193	33.195456
809.623139	47291.629211	33.200474
810.594373	47377.166028	33.205492
811.399911	47452.219689	33.210509
812.201512	47528.312360	33.215527
813.203823	47615.527112	33.220544
814.163538	47688.951235	33.225562
814.648312	47763.946846	33.230580
815.781350	47848.056110	33.235597
816.801031	47905.913005	33.240615
817.717863	47993.767977	33.245632
818.641300	48060.522835	33.250650
819.327872	48133.922869	33.255668
820.176780	48200.724827	33.260685
821.294357	48275.640823	33.265703
821.963281	48358.529546	33.270720
822.389665	48419.019458	33.275738
823.243044	48492.034717	33.280756
824.141852	48581.978030	33.285773
824.905181	48637.836586	33.290791
825.642057	48720.826629	33.295808
826.521996	48796.817631	33.300826
827.520122	48871.426998	33.305844
828.087427	48947.932257	33.310861
829.050253	49022.371172	33.315879
830.155732	49104.016909	33.320896
830.868953	49168.603721	33.325914
831.828683	49240.980352	33.330932
832.441680	49325.406606	33.335949
833.665641	49390.458843	33.340967
834.474248	49453.690409	33.345984
835.129053	49520.449348	33.351002
835.874742	49586.477758	33.356020
836.292695	49653.031913	33.361037
837.228230	49718.323747	33.366055
837.899529	49782.326211	33.371072
838.572084	49849.982908	33.376090
839.159769	49925.305773	33.381108
840.062803	50008.407919	33.386125
841.213095	50082.770949	33.391143
842.018976	50163.165947	33.396160
842.740188	50241.665593	33.401178
843.843248	50311.735896	33.406196
844.482433	50397.917632	33.411213
845.099533	50479.312903	33.416231
846.066130	50555.026233	33.421248
846.832073	50649.087829	33.426266
847.830016	50722.373258	33.431284
848.701442	50815.207124	33.436301
849.273322	50894.190991	33.441319
850.129721	50978.340175	33.446336
850.942602	51063.645404	33.451354
852.175455	51140.183534	33.456372
852.908353	51237.475597	33.461389
853.323538	51310.783597	33.466407
854.524889	51409.788265	33.471424
855.157243	51488.512653	33.476442
856.617343	51566.364011	33.481460
857.207038	51655.437871	33.486477
858.181735	51745.558638	33.491495
859.272477	51832.650597	33.496512
860.001120	51921.646855	33.501530
860.761199	51999.428452	33.506548
861.499118	52083.639546	33.511565
862.510731	52170.950878	33.516583
863.435059	52264.632791	33.521600
863.925991	52355.909815	33.526618
864.904779	52447.936551	33.531636
865.476015	52539.122819	33.536653
867.046381	52618.564483	33.541671
867.550740	52695.692283	33.546688
868.251972	52788.651798	33.551706
869.796549	52878.214120	33.556724
870.132360	52970.049167	33.561741
871.260320	53053.988099	33.566759
872.176832	53135.546585	33.571776
873.269301	53218.977473	33.576794
874.125149	53298.046628	33.581812
874.976514	53401.817559	33.586829
876.130729	53467.643740	33.591847
876.854550	53549.288411	33.596864
877.827965	53640.356259	33.601882
878.566406	53726.405570	33.606900
879.322692	53810.110468	33.611917
880.430736	53886.702230	33.616935
881.155076	53965.132397	33.621952
881.732123	54033.438677	33.626970
882.689320	54106.551826	33.631988
882.958380	54186.018089	33.637005
884.169472	54264.533063	33.642023
885.239305	54346.624967	33.647040
885.808265	54429.065244	33.652058
887.136592	54511.457650	33.657076
887.861389	54601.600857	33.662093
888.781303	54670.786119	33.667111
889.392383	54747.454284	33.672128
890.233261	54842.589534	33.677146
891.352007	54927.804357	33.682164
891.712700	55020.308667	33.687181
892.700535	55100.819821	33.692199
894.006242	55198.461845	33.697216
894.320379	55289.298796	33.702234
895.572283	55378.983175	33.707252
896.466823	55477.443387	33.712269
897.623563	55555.795809	33.717287
898.567323	55646.985738	33.722304
899.335789	55740.205328	33.727322
900.726970	55823.262871	33.732340
901.188207	55917.798074	33.737357
902.045522	56000.499440	33.742375
903.182346	56088.734597	33.747392
903.615398	56188.332719	33.752410
904.706180	56274.126479	33.757428
905.331449	56373.249917	33.762445
906.678402	56460.455890	33.767463
907.956305	56562.175533	33.772480
908.859892	56645.216531	33.777498
910.068324	56719.502905	33.782516
911.210778	56816.604997	33.787533
911.656151	56893.261158	33.792551
913.184784	56960.880818	33.797568
913.800297	57051.394411	33.802586
914.540082	57139.445246	33.807604
915.296089	57216.507913	33.812621
916.232679	57298.397497	33.817639
917.335794	57386.663192	33.822656
918.142928	57477.041047	33.827674
919.438856	57557.804401	33.832692
919.942418	57651.296818	33.837709
920.465789	57734.535820	33.842727
921.643542	57823.372613	33.847744
922.078641	57926.768201	33.852762
923.228211	58011.408391	33.857780
924.133127	58113.596890	33.862797
925.114063	58200.016939	33.867815
926.346228	58291.682368	33.872832
926.651420	58394.362478	33.877850
927.843539	58482.515060	33.882868
928.584018	58583.229527	33.887885
929.355086	58669.094774	33.892903
930.264681	58759.942473	33.897920
931.758459	58842.435337	33.902938
932.957828	58916.589925	33.907956
933.565472	59006.217686	33.912973
934.469533	59083.886538	33.917991
935.176477	59168.173058	33.923008
935.927689	59262.575041	33.928026
936.844537	59344.359994	33.933044
937.775257	59437.247231	33.938061
938.431586	59522.919982	33.943079
939.679562	59617.999315	33.948096
940.553343	59716.917988	33.953114
941.354207	59803.446765	33.958132
942.330056	59904.576114	33.963149
943.443502	59995.454239	33.968167
944.453285	60096.446619	33.973184
945.491773	60185.452636	33.978202
946.453571	60275.194328	33.983220
947.387267	60380.974365	33.988237
948.121582	60472.688706	33.993255
949.507430	60562.184329	33.998272
950.231946	60657.033337	34.003290
951.583874	60759.054713	34.008308
952.027303	60858.650978	34.013325
953.280462	60944.850996	34.018343
954.459648	61036.933053	34.023360
954.521088	61140.380642	34.028378
956.026689	61236.279756	34.033396
957.216295	61329.905648	34.038413
958.135102	61428.109421	34.043431
959.073672	61524.788585	34.048448
960.047581	61625.987525	34.053466
961.128206	61710.636531	34.058484
961.945975	61814.371664	34.063501
962.844428	61903.944919	34.068519
963.876001	62001.811657	34.073536
964.719666	62107.101028	34.078554
966.190177	62194.592125	34.083572
967.157365	62293.708454	34.088589
967.757368	62390.856435	34.093607
968.631712	62481.819372	34.098624
969.620946	62589.560818	34.103642
970.382148	62677.801725	34.108660
971.335088	62789.292097	34.113677
972.579287	62885.042251	34.118695
973.938082	62980.736763	34.123712
974.313371	63089.210303	34.128730
975.380823	63183.509037	34.133748
976.614190	63288.938772	34.138765
977.337764	63389.789084	34.143783
978.761258	63490.683316	34.148800
979.495205	63597.454244	34.153818
980.566822	63690.453750	34.158836
981.515361	63786.498659	34.163853
982.443591	63889.854939	34.168871
983.497818	63969.708589	34.173888
984.177515	64068.538865	34.178906
984.964476	64155.569849	34.183924
986.243934	64240.110105	34.188941
986.732680	64338.580558	34.193959
987.839703	64431.770696	34.198976
988.965096	64528.028064	34.203994
989.927481	64613.078348	34.209012
990.679780	64723.651904	34.214029
991.506412	64825.384016	34.219047
992.536087	64924.643086	34.224064
993.811553	65041.293718	34.229082
994.477043	65128.999053	34.234100
995.555213	65228.330938	34.239117
996.353308	65341.847416	34.244135
997.264814	65448.477271	34.249152
998.277830	65550.812080	34.254170
999.562177	65667.689351	34.259188
1000.202653	65779.752245	34.264205
1001.543448	65878.470900	34.269223
1002.812304	65992.307965	34.274240
1003.622155	66106.619841	34.279258
1004.807934	66206.126011	34.284276
1005.997111	66316.563440	34.289293
1007.287939	66420.655824	34.294311
1008.289176	66519.959251	34.299328
1009.250899	66624.158784	34.304346
1010.387433	66710.630922	34.309364
1011.387424	66821.126607	34.314381
1012.592272	66922.127412	34.319399
1013.438354	67013.154318	34.324416
1014.356786	67124.315369	34.329434
1015.470186	67218.724585	34.334452
1016.360849	67325.027016	34.339469
1017.065927	67433.261030	34.344487
1018.265225	67532.869807	34.349504
1019.402535	67648.566409	34.354522
1020.435430	67751.955244	34.359540
1021.657774	67860.564202	34.364557
1022.690600	67962.848637	34.369575
1023.723052	68059.536449	34.374592
1024.361004	68166.357495	34.379610
1025.560312	68282.123820	34.384628
1026.751293	68383.955724	34.389645
1027.556693	68491.048838	34.394663
1028.630727	68600.797414	34.399680
1029.268399	68711.791100	34.404698
1030.326097	68817.272784	34.409716
1031.629394	68925.723189	34.414733
1032.382766	69046.814993	34.419751
1033.890688	69148.044513	34.424768
1034.493238	69266.571389	34.429786
1035.546198	69371.886244	34.434804
1036.926439	69470.124140	34.439821
1038.011626	69577.930533	34.444839
1039.530554	69662.589136	34.449856
1040.421807	69762.087736	34.454874
1041.535264	69851.208952	34.459892
1042.847667	69939.243819	34.464909
1043.315739	70037.888705	34.469927
1044.372573	70119.526949	34.474944
1045.127279	70217.710151	34.479962
1045.979780	70319.751302	34.484980
1046.922881	70418.012945	34.489997
1048.172084	70525.261412	34.495015
1049.316752	70633.942377	34.500032
1049.933870	70739.788819	34.505050
1050.968040	70834.221819	34.510068
1052.149339	70943.062940	34.515085
1052.636362	71061.258875	34.520103
1053.839285	71170.116764	34.525120
1055.192162	71289.111459	34.530138
1055.886372	71402.423913	34.535156
1057.491454	71514.473751	34.540173
1058.619465	71626.277864	34.545191
1059.420793	71729.977276	34.550208
1060.194167	71858.735017	34.555226
1061.194700	71964.710271	34.560244
1062.292542	72092.609131	34.565261
1062.989594	72211.568362	34.570279
1064.859218	72331.485492	34.575296
1065.836833	72454.319193	34.580314
1066.483619	72574.065804	34.585332
1067.881080	72690.003500	34.590349
1068.993347	72810.972870	34.595367
1070.291192	72932.633820	34.600384
1071.251579	73053.205449	34.605402
1072.629869	73167.367017	34.610420
1073.640086	73281.695209	34.615437
1074.678166	73397.706828	34.620455
1076.054017	73501.406247	34.625472
1077.211283	73615.504431	34.630490
1078.208227	73725.894108	34.635508
1079.345833	73832.723240	34.640525
1080.411934	73952.095463	34.645543
1082.054956	74060.305179	34.650560
1082.862208	74178.759388	34.655578
1083.484961	74289.319118	34.660596
1084.707592	74390.412331	34.665613
1085.961314	74508.089697	34.670631
1087.054231	74620.301683	34.675648
1088.191967	74736.949801	34.680666
1089.393087	74841.650846	34.685684
1090.802044	74952.929684	34.690701
1091.439353	75068.698741	34.695719
1092.826681	75168.891249	34.700736
1093.994548	75286.334040	34.705754
1094.842081	75396.428045	34.710772
1096.124013	75496.866459	34.715789
1096.537845	75614.348932	34.720807
1097.884077	75705.178366	34.725824
1098.664934	75816.802029	34.730842
1099.758849	75921.494137	34.735860
1100.841575	76016.569621	34.740877
1101.734222	76130.717851	34.745895
1102.691306	76235.654547	34.750912
1103.863965	76352.780457	34.755930
1105.045267	76471.049603	34.760948
1105.973385	76579.108484	34.765965
1107.163298	76689.926127	34.770983
1108.155548	76806.565099	34.776000
1109.566562	76924.326340	34.781018
1110.650449	77034.467503	34.786036
1111.846031	77141.709447	34.791053
1112.846446	77267.678511	34.796071
1113.940230	77378.325588	34.801088
1114.445063	77496.531319	34.806106
1115.639569	77622.155685	34.811124
1117.251600	77749.585283	34.816141
1117.674820	77881.407887	34.821159
1119.089550	77999.888976	34.826176
1120.394599	78136.174339	34.831194
1121.442076	78255.871988	34.836212
1122.633728	78382.215714	34.841229
1123.436115	78513.406903	34.846247
1125.068015	78630.675136	34.851264
1125.907019	78773.195264	34.856282
1127.281314	78899.905022	34.861300
1128.595380	79019.571054	34.866317
1129.647383	79152.926294	34.871335
1130.954942	79269.503894	34.876352
1132.113631	79397.079051	34.881370
1132.743362	79517.255033	34.886388
1134.442834	79644.259001	34.891405
1135.859609	79766.119092	34.896423
1136.967777	79885.589024	34.901440
1137.963717	80015.564316	34.906458
1139.141038	80144.696144	34.911476
1140.555398	80259.163716	34.916493
1141.199949	80389.115061	34.921511
1142.288455	80506.910250	34.926528
1143.657350	80629.092791	34.931546
1145.142517	80758.811631	34.936564
1146.278345	80872.372359	34.941581
1147.216813	80999.246499	34.946599
1148.825582	81111.835680	34.951616
1149.867851	81237.323001	34.956634
1150.802862	81358.346136	34.961652
1152.532404	81463.667169	34.966669
1153.534896	81584.529170	34.971687
1154.937372	81691.894691	34.976704
1156.087733	81811.406942	34.981722
1156.747911	81925.851922	34.986740
1158.122221	82038.837425	34.991757
1159.143512	82160.357241	34.996775
1160.068100	82267.593101	35.001792
1160.920968	82377.736341	35.006810
1161.925154	82484.385364	35.011828
1163.431633	82585.240012	35.016845
1164.176973	82699.991783	35.021863
1165.089903	82823.094210	35.026880
1166.527797	82935.138788	35.031898
1167.286513	83057.489500	35.036916
1168.602742	83178.241281	35.041933
1169.667982	83306.297838	35.046951
1170.702532	83420.248896	35.051968
1171.894517	83543.728437	35.056986
1172.916225	83687.062445	35.062004
1174.263085	83812.839214	35.067021
1175.202032	83952.312604	35.072039
1176.234664	84090.273609	35.077056
1177.482770	84210.460484	35.082074
1178.200614	84354.018046	35.087092
1179.607994	84502.012831	35.092109
1180.774993	84644.305983	35.097127
1182.658698	84778.361574	35.102144
1183.649720	84923.788987	35.107162
1184.659215	85063.511390	35.112180
1186.193312	85194.084498	35.117197
1187.243369	85340.434820	35.122215
1188.611491	85473.211070	35.127232
1190.035639	85607.736995	35.132250
1190.871635	85748.718124	35.137268
1192.491184	85869.961852	35.142285
1193.895481	86017.929760	35.147303
1195.345044	86141.263352	35.152320
1196.562069	86263.673530	35.157338
1197.692979	86397.169825	35.162356
1199.102305	86528.327390	35.167373
1200.121452	86653.622996	35.172391
1201.156709	86784.221939	35.177408
1202.531712	86916.708892	35.182426
1203.599556	87048.701702	35.187444
1205.130367	87180.280251	35.192461
1206.105797	87316.823224	35.197479
1207.103781	87444.573957	35.202496
1208.802766	87578.815653	35.207514
1209.703427	87720.406532	35.212532
1210.838619	87843.268740	35.217549
1212.172128	87972.581755	35.222567
1213.268715	88104.468975	35.227584
1214.210954	88240.042923	35.232602
1215.623020	88382.189197	35.237620
1216.744720	88518.153720	35.242637
1217.564621	88657.202482	35.247655
1219.062425	88791.407833	35.252672
1220.728673	88923.519344	35.257690
1221.334863	89076.384402	35.262708
1222.546460	89208.032405	35.267725
1223.864390	89350.623708	35.272743
1225.298803	89468.363117	35.277760
1226.683330	89587.451789	35.282778
1227.844260	89704.356922	35.287796
1229.034643	89828.638213	35.292813
1230.454972	89949.860721	35.297831
1231.570050	90082.452689	35.302848
1232.757932	90195.106334	35.307866
1233.281506	90321.621384	35.312884
1234.641398	90451.558438	35.317901
1236.023238	90587.874006	35.322919
1236.924771	90723.507865	35.327936
1238.308864	90865.111959	35.332954
1239.386939	91003.748869	35.337972
1240.707656	91143.631946	35.342989
1241.694443	91283.214834	35.348007
1242.954019	91434.076188	35.353024
1244.651034	91564.004192	35.358042
1245.431697	91708.954186	35.363060
1247.162238	91859.933325	35.368077
1248.249520	92000.832972	35.373095
1249.548923	92144.685081	35.378112
1251.029070	92286.428534	35.383130
1251.781696	92437.402657	35.388148
1253.461961	92580.513973	35.393165
1254.560648	92728.361172	35.398183
1255.945551	92869.661789	35.403200
1257.401420	93025.404669	35.408218
1258.370062	93176.596164	35.413236
1259.392172	93316.736574	35.418253
1261.349347	93467.564166	35.423271
1262.417170	93614.618886	35.428288
1264.103828	93754.454002	35.433306
1265.237999	93900.064238	35.438324
1266.838429	94038.751002	35.443341
1268.181272	94178.991337	35.448359
1268.989970	94321.322613	35.453376
1270.589741	94456.128298	35.458394
1271.591506	94610.537572	35.463412
1273.205055	94752.376765	35.468429
1274.500322	94893.615927	35.473447
1275.898399	95028.918894	35.478464
1277.309519	95163.056693	35.483482
1278.463760	95320.546172	35.488500
1279.835645	95449.789537	35.493517
1281.004864	95594.525957	35.498535
1282.120871	95727.657645	35.503552
1283.429581	95853.623973	35.508570
1284.807109	96010.311037	35.513588
1285.854062	96145.347602	35.518605
1287.574322	96283.048696	35.523623
1288.550034	96431.952089	35.528640
1289.912758	96579.580345	35.533658
1290.869039	96723.282437	35.538676
1292.558122	96861.890316	35.543693
1293.498340	97008.291685	35.548711
1294.914258	97143.515949	35.553728
1296.094661	97257.908312	35.558746
1297.208249	97385.628597	35.563764
1298.617576	97518.521763	35.568781
1299.428548	97655.249672	35.573799
1300.585081	97796.585991	35.578816
1302.075941	97942.848910	35.583834
1302.875312	98084.186849	35.588852
1304.572038	98220.132050	35.593869
1305.839618	98366.673586	35.598887
1306.896588	98517.773024	35.603904
1308.659948	98651.299786	35.608922
1309.829317	98806.761263	35.613940
1310.498118	98954.667073	35.618957
1312.048120	99106.248768	35.623975
1313.465213	99262.312953	35.628992
1314.755288	99420.119279	35.634010
1316.173056	99577.684951	35.639028
1317.503841	99723.396296	35.644045
1318.691895	99878.545711	35.649063
1320.019340	100060.943256	35.654080
1321.711327	100211.857990	35.659098
1322.761442	100369.841829	35.664116
1324.072019	100525.222870	35.669133
1326.023228	100685.400334	35.674151
1327.445799	100837.747625	35.679168
1328.833560	100987.121326	35.684186
1329.727763	101138.029713	35.689204
1331.558114	101285.746843	35.694221
1332.528654	101450.470296	35.699239
1334.041758	101598.923197	35.704256
1335.586909	101748.396996	35.709274
1336.570345	101908.496285	35.714292
1337.978327	102057.120675	35.719309
1339.854979	102213.530345	35.724327
1341.076084	102364.774370	35.729344
1342.512961	102523.584574	35.734362
1343.515702	102675.580338	35.739380
1345.069943	102825.091222	35.744397
1346.673583	102985.263822	35.749415
1347.580327	103144.630750	35.754432
1349.371738	103296.619083	35.759450
1350.660778	103453.478463	35.764468
1352.141251	103599.677532	35.769485
1353.142216	103753.249876	35.774503
1355.001705	103909.996316	35.779520
1356.011946	104053.267130	35.784538
1357.402221	104221.006108	35.789556
1359.008811	104366.424185	35.794573
1360.265313	104510.171206	35.799591
1361.326223	104667.802652	35.804608
1362.967654	104822.457192	35.809626
1364.658423	104975.491182	35.814644
1365.671583	105130.570329	35.819661
1366.972808	105273.568123	35.824679
1368.053158	105416.703136	35.829696
1369.542304	105552.559599	35.834714
1370.446111	105704.875346	35.839732
1371.779155	105838.150908	35.844749
1373.434995	105976.761520	35.849767
1373.994599	106133.317886	35.854784
1375.685509	106283.271896	35.859802
1376.872718	106443.053079	35.864820
1378.467768	106588.372651	35.869837
1379.775636	106746.915239	35.874855
1380.836115	106908.561335	35.879872
1382.368133	107059.621353	35.884890
1383.804054	107232.393039	35.889908
1385.237752	107394.926093	35.894925
1386.462919	107550.626441	35.899943
1388.026068	107719.065032	35.904960
1389.681273	107873.838373	35.909978
1391.058196	108035.131608	35.914996
1392.345494	108199.022454	35.920013
1393.849463	108361.816670	35.925031
1395.440289	108526.262765	35.930048
1397.756749	108666.404171	35.935066
1399.176875	108818.765157	35.940084
1400.626579	108967.856454	35.945101
1402.577576	109099.817635	35.950119
1403.830871	109255.302938	35.955136
1404.962260	109394.731774	35.960154
1406.435334	109546.936996	35.965172
1407.846941	109695.007090	35.970189
1409.342070	109835.538943	35.975207
1411.103677	109969.585715	35.980224
1414.077178	110057.879907	35.985242
1413.877377	110246.731752	35.990260
1416.046084	110353.435030	35.995277
1416.722975	110512.957009	36.000295
1417.762598	110661.459185	36.005312
1419.778479	110775.461514	36.010330
1420.529899	110936.132749	36.015348
1421.592900	111098.844382	36.020365
1423.480329	111242.702120	36.025383
1424.262466	111410.169910	36.030400
1426.010279	111546.221424	36.035418
1427.198510	111710.784542	36.040436
1428.381995	111878.217042	36.045453
1429.627864	112032.961491	36.050471
1431.008756	112201.941012	36.055488
1432.360273	112370.204704	36.060506
1433.995357	112540.247592	36.065524
1435.365058	112708.903164	36.070541
1436.694681	112873.844000	36.075559
1438.090467	113049.511761	36.080576
1439.697558	113209.397053	36.085594
1441.068682	113393.351364	36.090612
1442.545570	113572.048543	36.095629
1444.294112	113725.362563	36.100647
1445.512005	113881.211787	36.105664
1446.938232	114022.069567	36.110682
1448.048329	114175.772670	36.115700
1449.591663	114335.751251	36.120717
1451.322600	114484.894436	36.125735
1452.308417	114646.565265	36.130752
1453.798290	114791.538591	36.135770
1455.374941	114955.700498	36.140788
1457.298302	115097.346301	36.145805
1459.448653	115233.607184	36.150823
1461.221415	115387.161730	36.155840
1462.242742	115521.191458	36.160858
1463.899967	115669.448022	36.165876
1465.212811	115805.104328	36.170893
1466.886680	115950.523564	36.175911
1468.120606	116118.381534	36.180928
1469.506835	116263.196153	36.185946
1470.844141	116408.380251	36.190964
1472.031848	116575.647110	36.195981
1473.695294	116730.797307	36.200999
1474.984652	116894.137347	36.206016
1476.344100	117062.285488	36.211034
1477.926049	117226.296607	36.216052
1478.926953	117384.664778	36.221069
1480.580549	117548.679239	36.226087
1482.034928	117733.063376	36.231104
1483.559325	117891.997318	36.236122
1485.151789	118061.298990	36.241140
1486.405770	118238.120614	36.246157
1487.906682	118409.775513	36.251175
1489.311128	118592.438839	36.256192
1491.032709	118765.276741	36.261210
1492.530060	118941.792244	36.266228
1493.931095	119123.503748	36.271245
1495.084053	119299.120284	36.276263
1496.646524	119484.329227	36.281280
1498.212803	119667.518964	36.286298
1500.372644	119846.892422	36.291316
1501.466303	120029.969837	36.296333
1503.296515	120207.777126	36.301351
1504.590320	120376.020565	36.306368
1506.331404	120551.881373	36.311386
1507.866023	120736.096799	36.316404
1509.352873	120918.294761	36.321421
1511.212553	121082.020192	36.326439
1512.553707	121256.796775	36.331456
1514.226240	121434.358814	36.336474
1515.942397	121594.234771	36.341492
1517.339559	121779.125260	36.346509
1519.018406	121950.939826	36.351527
1520.394678	122121.017780	36.356544
1521.743216	122294.064921	36.361562
1523.423584	122463.045537	36.366580
1524.880081	122637.559623	36.371597
1526.575174	122799.802000	36.376615
1527.491229	122959.572675	36.381632
1529.268454	123115.281119	36.386650
1530.457363	123272.920481	36.391668
1531.650073	123439.704935	36.396685
1533.216756	123605.595066	36.401703
1534.599939	123761.724533	36.406720
1536.339211	123932.909012	36.411738
1537.688990	124100.622594	36.416756
1539.205616	124274.238536	36.421773
1540.707474	124455.369098	36.426791
1542.320438	124626.375408	36.431808
1543.942696	124800.699958	36.436826
1545.561014	124973.582270	36.441844
1546.791376	125154.887335	36.446861
1548.695370	125331.729233	36.451879
1550.370850	125511.775306	36.456896
1552.117215	125683.096462	36.461914
1553.764979	125858.057133	36.466932
1555.165878	126034.844210	36.471949
1557.010425	126207.027111	36.476967
1558.043501	126390.246523	36.481984
1559.819004	126567.218231	36.487002
1561.375524	126746.569350	36.492020
1562.900921	126930.917592	36.497037
1564.892987	127109.948559	36.502055
1566.279656	127296.702814	36.507072
1568.050208	127473.288481	36.512090
1569.565271	127655.426386	36.517108
1570.828477	127854.352519	36.522125
1572.535946	128024.237743	36.527143
1573.846392	128218.649189	36.532160
1575.075209	128397.151053	36.537178
1576.954803	128584.317140	36.542196
1578.699284	128788.848950	36.547213
1580.396973	128979.302378	36.552231
1582.174289	129165.804550	36.557248
1583.664349	129355.064691	36.562266
1585.477556	129538.763901	36.567284
1586.943489	129727.409642	36.572301
1588.455909	129916.391336	36.577319
1590.163049	130105.140677	36.582336
1591.480173	130304.620589	36.587354
1593.157697	130480.594093	36.592372
1594.405023	130674.792030	36.597389
1596.165328	130870.620185	36.602407
1597.823915	131066.693913	36.607424
1599.588114	131257.937827	36.612442
1601.411528	131450.731992	36.617460
1602.738503	131642.922168	36.622477
1604.586901	131835.170197	36.627495
1606.103093	132026.838808	36.632512
1607.482848	132212.993635	36.637530
1609.626035	132401.853833	36.642548
1610.859528	132599.893551	36.647565
1612.088587	132787.292406	36.652583
1614.149178	132962.384308	36.657600
1615.661825	133137.881077	36.662618
1617.411023	133309.413528	36.667636
1618.769206	133486.242024	36.672653
1620.796643	133652.144659	36.677671
1622.339821	133828.679807	36.682688
1623.647896	133998.335176	36.687706
1625.002910	134172.621598	36.692724
1626.741899	134357.339564	36.697741
1628.475995	134530.262845	36.702759
1630.070708	134727.563005	36.707776
1631.189122	134909.088604	36.712794
1633.218075	135092.865579	36.717812
1634.795562	135285.940111	36.722829
1636.502195	135475.194011	36.727847
1638.233915	135657.513887	36.732864
1639.630552	135862.101294	36.737882
1641.448468	136043.636939	36.742900
1642.937677	136245.221838	36.747917
1644.882508	136425.751314	36.752935
1646.686656	136625.159960	36.757952
1647.981606	136825.651919	36.762970
1649.562941	137011.945117	36.767988
1651.279639	137220.406853	36.773005
1653.056587	137421.434591	36.778023
1654.431000	137612.149036	36.783040
1656.124982	137822.848967	36.788058
1658.065654	138021.168252	36.793076
1659.623025	138225.341092	36.798093
1661.506640	138417.057029	36.803111
1662.997147	138637.540323	36.808128
1664.951558	138829.488463	36.813146
1666.674337	139026.581800	36.818164
1668.365713	139226.583537	36.823181
1670.463359	139427.041690	36.828199
1672.147090	139630.633823	36.833216
1673.797869	139834.511385	36.838234
1675.512369	140015.771040	36.843252
1677.127632	140215.157810	36.848269
1678.856824	140412.107177	36.853287
1680.315171	140613.333811	36.858304
1682.244474	140807.098269	36.863322
1683.864749	140998.403652	36.868340
1685.517789	141207.790549	36.873357
1687.262287	141404.705941	36.878375
1688.792828	141603.519663	36.883392
1690.605579	141802.670091	36.888410
1692.577763	141998.159031	36.893428
1694.049746	142198.849041	36.898445
1695.958716	142388.342947	36.903463
1697.879973	142584.730936	36.908480
1699.343885	142775.387914	36.913498
1701.587575	142975.846408	36.918516
1702.868081	143165.584347	36.923533
1704.652107	143353.912657	36.928551
1706.385729	143526.102476	36.933568
1707.924054	143704.167368	36.938586
1709.525904	143872.970521	36.943604
1710.984904	144051.404909	36.948621
1712.589471	144231.059366	36.953639
1713.890745	144392.612258	36.958656
1715.555973	144586.011641	36.963674
1717.136172	144767.270147	36.968692
1718.661266	144973.039901	36.973709
1720.725008	145164.034658	36.978727
1722.496998	145350.488380	36.983744
1724.002141	145554.908859	36.988762
1725.733157	145749.471167	36.993780
1727.427251	145945.967257	36.998797
1729.266736	146152.062442	37.003815
1731.265709	146351.998515	37.008832
1732.612287	146563.866145	37.013850
1734.470415	146754.256762	37.018868
1736.468984	146956.174196	37.023885
1737.975382	147173.243108	37.028903
1739.704321	147372.493295	37.033920
1741.130731	147584.076197	37.038938
1742.987453	147784.246729	37.043956
1744.755314	148009.126574	37.048973
1746.757183	148213.751586	37.053991
1748.602706	148422.941003	37.059008
1750.347475	148628.877168	37.064026
1752.459705	148836.670521	37.069044
1754.010478	149049.561771	37.074061
1755.795497	149254.899741	37.079079
1757.954982	149458.341377	37.084096
1759.273389	149675.444434	37.089114
1761.160334	149888.642808	37.094132
1762.947868	150108.970385	37.099149
1764.772580	150315.259590	37.104167
1766.787547	150531.598554	37.109184
1767.977998	150750.085609	37.114202
1770.150462	150954.688236	37.119220
1771.962798	151166.220692	37.124237
1773.680575	151386.213001	37.129255
1776.182423	151588.434567	37.134272
1777.565932	151801.040762	37.139290
1779.462514	152001.928350	37.144308
1781.392412	152215.147767	37.149325
1783.354417	152418.296905	37.154343
1785.188095	152626.995432	37.159360
1786.714734	152847.877294	37.164378
1788.357286	153037.971437	37.169396
1790.364762	153250.703421	37.174413
1792.034132	153456.796100	37.179431
1793.830936	153661.272297	37.184448
1795.625876	153876.070615	37.189466
1797.159428	154087.298317	37.194484
1798.993642	154300.470219	37.199501
1800.834453	154508.659549	37.204519
1802.844644	154693.962768	37.209536
1804.138993	154896.053825	37.214554
1806.095271	155079.212253	37.219572
1807.603897	155265.003972	37.224589
1809.332837	155475.055532	37.229607
1811.388749	155665.263763	37.234624
1812.808526	155875.125968	37.239642
1814.364168	156066.265395	37.244660
1816.206515	156271.853313	37.249677
1818.387249	156479.493600	37.254695
1819.942170	156687.373974	37.259712
1821.620230	156901.423884	37.264730
1823.460605	157108.919138	37.269748
1825.511677	157322.975860	37.274765
1826.967316	157540.919816	37.279783
1829.099427	157752.886789	37.284800
1830.729107	157980.125893	37.289818
1832.566898	158204.797361	37.294836
1834.207330	158421.411437	37.299853
1835.854429	158650.338670	37.304871
1838.145638	158871.417258	37.309888
1839.610519	159109.785503	37.314906
1841.461067	159329.009459	37.319924
1843.375515	159570.834752	37.324941
1845.180795	159806.503378	37.329959
1847.355422	160032.870425	37.334976
1849.239704	160273.285047	37.339994
1850.908308	160500.407519	37.345012
1853.112194	160736.691187	37.350029
1854.605055	160964.656136	37.355047
1856.903098	161202.639951	37.360064
1858.433362	161444.894116	37.365082
1860.742361	161676.957046	37.370100
1862.873253	161911.548063	37.375117
1864.650462	162144.789070	37.380135
1866.891060	162366.239926	37.385152
1868.577459	162602.212246	37.390170
1870.865350	162826.118734	37.395188
1873.019987	163065.418559	37.400205
1874.556716	163278.908190	37.405223
1876.730710	163488.975154	37.410240
1878.078774	163719.719923	37.415258
1880.465316	163940.573853	37.420276
1882.266004	164159.771915	37.425293
1884.329793	164392.728240	37.430311
1886.446306	164611.777418	37.435328
1888.149177	164830.043809	37.440346
1889.941648	165053.154811	37.445364
1891.843146	165282.160109	37.450381
1893.567372	165486.843563	37.455399
1895.679903	165712.786790	37.460416
1897.305737	165934.141235	37.465434
1899.494114	166151.628105	37.470452
1901.583461	166371.173977	37.475469
1903.418283	166589.505881	37.480487
1905.757539	166783.203819	37.485504
1907.374847	166977.867139	37.490522
1909.052168	167176.808996	37.495540
1910.813475	167358.641011	37.500557
1912.782531	167557.931773	37.505575
1914.735163	167751.049193	37.510592
1916.321760	167955.095751	37.515610
1917.695037	168169.463922	37.520628
1919.426202	168366.665799	37.525645
1921.345765	168584.539178	37.530663
1923.184525	168802.946676	37.535680
1924.883887	169029.787174	37.540698
1927.132575	169249.946008	37.545716
1928.815264	169469.155816	37.550733
1930.718318	169692.352864	37.555751
1933.075740	169917.153449	37.560768
1934.774171	170146.233152	37.565786
1936.623500	170386.262486	37.570804
1939.024901	170614.282046	37.575821
1940.578242	170844.923753	37.580839
1942.694800	171071.570500	37.585856
1944.666349	171307.666495	37.590874
1946.454688	171542.638652	37.595892
1948.371028	171773.494614	37.600909
1950.130027	172027.489299	37.605927
1952.471760	172262.923401	37.610944
1954.264741	172495.388826	37.615962
1956.119204	172742.396024	37.620980
1958.683218	172979.118396	37.625997
1960.554734	173221.546406	37.631015
1962.698731	173456.917490	37.636032
1964.734873	173703.292906	37.641050
1966.579237	173930.367124	37.646068
1968.974174	174161.579647	37.651085
1970.947826	174411.927318	37.656103
1973.549277	174630.347709	37.661120
1975.034805	174869.802280	37.666138
1976.999911	175093.413271	37.671156
1979.457738	175323.620259	37.676173
1981.335110	175565.744290	37.681191
1983.348145	175799.665517	37.686208
1985.552575	176026.846583	37.691226
1987.444734	176247.950875	37.696244
1989.658651	176475.805307	37.701261
1991.115625	176714.006553	37.706279
1993.861443	176932.175310	37.711296
1995.767101	177154.804729	37.716314
1997.437471	177378.538375	37.721332
1999.999066	177593.428577	37.726349
2002.089410	177811.515665	37.731367
2004.127595	178029.003191	37.736384
2005.901032	178248.018250	37.741402
2007.914882	178473.834698	37.746420
2009.821058	178687.286684	37.751437
2011.832948	178903.095506	37.756455
2013.983606	179094.840830	37.761472
2015.779134	179285.577629	37.766490
2017.320649	179492.659016	37.771508
2019.810858	179685.571138	37.776525
2021.399308	179888.853429	37.781543
2023.355292	180083.806012	37.786560
2025.359880	180284.232872	37.791578
2027.456880	180490.380887	37.796596
2028.972997	180688.844407	37.801613
2030.623417	180916.089090	37.806631
2033.156036	181126.700624	37.811648
2034.731029	181345.027196	37.816666
2036.637659	181580.824524	37.821684
2038.941636	181794.330407	37.826701
2040.992586	182022.024865	37.831719
2043.128343	182246.433474	37.836736
2045.008401	182476.606257	37.841754
2047.062630	182707.577362	37.846772
2049.170685	182944.225590	37.851789
2050.904913	183191.859258	37.856807
2052.981337	183418.617960	37.861824
2055.048636	183655.517546	37.866842
2057.001654	183894.986969	37.871860
2059.370122	184133.402037	37.876877
2061.360005	184384.377020	37.881895
2063.590556	184622.626243	37.886912
2065.799876	184867.567228	37.891930
2067.973027	185114.431341	37.896948
2070.122695	185343.370710	37.901965
2072.233131	185600.665247	37.906983
2074.628210	185834.072846	37.912000
2076.760852	186074.654712	37.917018
2078.593792	186314.079895	37.922036
2081.042223	186545.312773	37.927053
2083.045140	186782.670425	37.932071
2085.398559	187009.745844	37.937088
2087.735794	187239.603994	37.942106
2089.765357	187477.240167	37.947124
2092.309535	187703.260859	37.952141
2094.472203	187938.670248	37.957159
2096.306145	188158.283215	37.962176
2098.599259	188379.296413	37.967194
2101.203322	188610.159588	37.972212
2103.425405	188826.795398	37.977229
2105.357643	189052.792789	37.982247
2107.530146	189267.408057	37.987264
2109.664132	189482.499950	37.992282
2111.910085	189699.326329	37.997300
2114.427190	189917.189370	38.002317
2116.075592	190134.264804	38.007335
2118.437754	190339.045079	38.012352
2120.905408	190544.177524	38.017370
2122.967516	190758.855092	38.022388
2124.988115	190956.725017	38.027405
2127.476797	191153.239738	38.032423
2129.624278	191341.534977	38.037440
2131.432327	191513.919699	38.042458
2133.064825	191694.988071	38.047476
2135.535373	191868.741108	38.052493
2137.538229	192049.548995	38.057511
2139.322690	192233.539569	38.062528
2141.178216	192423.928559	38.067546
2143.135117	192611.560922	38.072564
2145.157863	192807.280529	38.077581
2147.487294	193009.488253	38.082599
2149.546101	193203.020817	38.087616
2151.455659	193405.867866	38.092634
2152.957872	193625.812198	38.097652
2155.264845	193823.622887	38.102669
2157.575506	194053.924004	38.107687
2159.701511	194273.023440	38.112704
2162.085329	194482.348476	38.117722
2164.083521	194703.881467	38.122740
2166.556228	194923.867926	38.127757
2168.439818	195145.256034	38.132775
2170.706785	195363.589027	38.137792
2173.010207	195589.075396	38.142810
2175.194319	195816.510859	38.147828
2177.750266	196029.749475	38.152845
2179.871183	196247.094045	38.157863
2181.727355	196465.446121	38.162880
2184.359879	196693.131642	38.167898
2185.857884	196921.924634	38.172916
2188.863015	197156.800347	38.177933
2190.936494	197375.236015	38.182951
2193.243808	197594.130513	38.187968
2195.630091	197818.737686	38.192986
2197.393573	198045.094616	38.198004
2200.148469	198269.264476	38.203021
2202.207147	198498.559278	38.208039
2204.110645	198723.005706	38.213056
2206.925969	198944.985706	38.218074
2209.261640	199173.719089	38.223092
2211.606035	199391.168164	38.228109
2213.545721	199617.732308	38.233127
2215.740633	199843.571513	38.238144
2218.219169	200063.083667	38.243162
2220.065553	200281.529207	38.248180
2222.691943	200509.092474	38.253197
2224.585787	200736.785559	38.258215
2226.637173	200959.643897	38.263232
2228.967130	201191.966186	38.268250
2231.067521	201423.615039	38.273268
2233.481025	201639.843592	38.278285
2235.578164	201877.156085	38.283303
2237.908160	202102.805483	38.288320
2240.270702	202340.319041	38.293338
2242.158515	202559.465185	38.298356
2244.414480	202796.439065	38.303373
2246.260878	203024.796443	38.308391
2248.756202	203237.222813	38.313408
2250.952872	203446.346196	38.318426
2252.879998	203656.058926	38.323444
2255.108620	203864.899521	38.328461
2256.636526	204088.348400	38.333479
2259.079684	204302.157960	38.338496
2260.995062	204522.995610	38.343514
2262.908678	204761.517157	38.348532
2265.259010	204992.658651	38.353549
2267.345661	205241.043418	38.358567
2269.764051	205479.589428	38.363584
2272.370259	205721.800653	38.368602
2273.752994	205967.799366	38.373620
2276.313528	206213.840843	38.378637
2279.035621	206464.681598	38.383655
2281.226891	206717.080141	38.388672
2283.597631	206967.712152	38.393690
2285.879651	207230.571443	38.398708
2288.252135	207469.335875	38.403725
2290.283190	207734.534889	38.408743
2292.427355	207990.602329	38.413760
2294.992969	208248.850998	38.418778
2297.247848	208521.952198	38.423796
2299.775875	208780.526452	38.428813
2302.056061	209046.605713	38.433831
2304.837726	209303.466222	38.438848
2307.446054	209566.626632	38.443866
2309.423684	209823.400967	38.448884
2312.257962	210076.904836	38.453901
2314.528988	210334.117168	38.458919
2317.223909	210594.906881	38.463936
2319.786748	210847.504758	38.468954
2321.702364	211102.440641	38.473972
2324.187600	211334.232394	38.478989
2326.767191	211605.962593	38.484007
2328.734042	211855.815184	38.489024
2331.531057	212102.147416	38.494042
2333.648971	212364.724358	38.499060
2336.383988	212616.540183	38.504077
2338.623596	212866.467694	38.509095
2340.490505	213118.880135	38.514112
2343.159916	213374.213308	38.519130
2345.436739	213631.590263	38.524148
2347.894309	213885.397411	38.529165
2350.279656	214137.617291	38.534183
2352.460850	214389.045251	38.539200
2355.056948	214639.126079	38.544218
2357.132220	214909.489872	38.549236
2359.892614	215156.689956	38.554253
2362.432364	215405.614512	38.559271
2364.353111	215661.874958	38.564288
2366.974935	215918.279145	38.569306
2369.011446	216181.506128	38.574324
2371.470471	216427.552433	38.579341
2373.589298	216683.518653	38.584359
2375.559814	216920.185320	38.589376
2378.229146	217138.662199	38.594394
2380.265601	217387.267393	38.599412
2382.152400	217628.583956	38.604429
2384.695972	217869.263969	38.609447
2386.673958	218114.224357	38.614464
2389.048523	218363.274542	38.619482
2391.460982	218611.786323	38.624500
2393.806752	218863.394856	38.629517
2396.219236	219131.982067	38.634535
2398.524880	219396.448019	38.639552
2400.840993	219649.486027	38.644570
2402.746490	219924.746230	38.649588
2405.607223	220185.597275	38.654605
2408.065941	220471.881721	38.659623
2410.479349	220738.227268	38.664640
2412.562384	221020.065889	38.669658
2415.189126	221302.352663	38.674676
2417.295730	221577.320434	38.679693
2420.146156	221861.770462	38.684711
2422.164308	222145.997947	38.689728
2425.022300	222429.763228	38.694746
2427.356119	222712.279406	38.699764
2430.036054	223004.353754	38.704781
2432.894298	223286.128620	38.709799
2434.710129	223636.789098	38.714816
2437.494136	223921.917473	38.719834
2440.093158	224210.136335	38.724852
2442.328935	224494.236256	38.729869
2445.114413	224791.125603	38.734887
2447.466126	225078.942356	38.739904
2450.460307	225360.195081	38.744922
2452.673794	225655.235468	38.749940
2455.129702	225939.038889	38.754957
2457.876437	226217.603706	38.759975
2460.314797	226510.033804	38.764992
2463.036209	226793.404419	38.770010
2465.115449	227085.436307	38.775028
2467.876651	227364.891508	38.780045
2470.260574	227654.515201	38.785063
2472.841930	227949.898988	38.790080
2475.349120	228235.924193	38.795098
2477.501812	228524.419209	38.800116
2479.962085	228822.948947	38.805133
2482.598213	229107.483558	38.810151
2485.341455	229404.725974	38.815168
2487.853490	229693.777390	38.820186
2490.267120	229988.940639	38.825204
2492.894274	230282.394799	38.830221
2495.393210	230574.651160	38.835239
2497.537389	230860.945505	38.840256
2500.131874	231159.766501	38.845274
2502.690870	231453.082826	38.850292
2504.741574	231749.985493	38.855309
2507.827792	232030.013331	38.860327
2509.881998	232302.992590	38.865344
2512.372601	232567.141231	38.870362
2514.513017	232835.206575	38.875380
2516.824268	233105.048846	38.880397
2519.388450	233379.144052	38.885415
2521.683559	233657.955918	38.890432
2524.310938	233935.801586	38.895450
2526.549841	234225.545175	38.900468
2528.731996	234515.095413	38.905485
2531.442527	234800.905390	38.910503
2533.927604	235104.683213	38.915520
2536.467491	235396.109570	38.920538
2538.762040	235699.360586	38.925556
2541.140339	236002.650017	38.930573
2543.709266	236312.793186	38.935591
2545.949229	236630.202667	38.940608
2548.940152	236935.480422	38.945626
2551.513365	237256.242419	38.950644
2554.106807	237569.560246	38.955661
2556.856695	237884.682925	38.960679
2559.118940	238213.065965	38.965696
2561.876414	238519.985324	38.970714
2564.583307	238849.874549	38.975732
2567.193571	239164.362609	38.980749
2570.095494	239476.468577	38.985767
2572.422083	239810.865771	38.990784
2575.250134	240127.557134	38.995802
2577.820341	240451.808525	39.000820
2580.440354	240785.069837	39.005837
2583.327268	241100.992507	39.010855
2585.986824	241426.400798	39.015872
2588.557975	241740.800386	39.020890
2591.079932	242065.419392	39.025908
2593.679113	242391.271623	39.030925
2596.459573	242713.260560	39.035943
2598.787086	243048.250805	39.040960
2601.830399	243365.424515	39.045978
2604.571556	243689.708183	39.050996
2607.130002	244018.923893	39.056013
2609.984868	244338.669886	39.061031
2612.553920	244663.237239	39.066048
2615.427556	244988.493740	39.071066
2617.823932	245320.354611	39.076084
2620.358311	245634.540914	39.081101
2623.280664	245956.286702	39.086119
2625.756106	246288.645387	39.091136
2628.341048	246609.633300	39.096154
2631.110598	246931.786533	39.101172
2633.572045	247255.564160	39.106189
2636.376354	247574.004762	39.111207
2638.859787	247902.149313	39.116224
2641.563771	248226.424065	39.121242
2644.338838	248553.787202	39.126260
2646.890338	248872.854832	39.131277
2649.916510	249188.952168	39.136295
2652.237535	249489.616198	39.141312
2654.290984	249775.437945	39.146330
2657.138668	250072.006213	39.151348
2659.335801	250375.434887	39.156365
2661.987277	250675.464539	39.161383
2664.118356	250981.521148	39.166400
2666.826231	251295.082038	39.171418
2669.469278	251616.248885	39.176436
2671.618728	251939.704472	39.181453
2674.612384	252255.279372	39.186471
2677.066745	252585.444718	39.191488
2679.440204	252918.773318	39.196506
2682.340276	253253.797239	39.201524
2684.753277	253597.433987	39.206541
2687.357214	253934.004750	39.211559
2689.985531	254286.270724	39.216576
2693.066349	254636.230269	39.221594
2695.198113	254983.343305	39.226612
2697.982222	255349.456069	39.231629
2700.924400	255707.669744	39.236647
2703.322255	256077.299678	39.241664
2706.165694	256435.758845	39.246682
2708.995598	256802.933764	39.251700
2711.702515	257163.193907	39.256717
2714.579712	257532.115294	39.261735
2717.220441	257918.373831	39.266752
2720.355575	258279.025127	39.271770
2722.992625	258651.644263	39.276788
2725.701466	259030.095192	39.281805
2728.622187	259390.502641	39.286823
2731.730311	259767.468870	39.291840
2734.293444	260136.037441	39.296858
2737.004408	260501.001308	39.301876
2739.752560	260881.684093	39.306893
2742.879891	261251.866766	39.311911
2745.436511	261630.650255	39.316928
2748.484533	262001.659314	39.321946
2751.367965	262372.415452	39.326964
2753.745602	262757.249152	39.331981
2756.816240	263113.700030	39.336999
2759.635457	263498.159811	39.342016
2762.406403	263876.353109	39.347034
2765.414962	264240.791518	39.352052
2767.941320	264615.417077	39.357069
2771.024288	264978.116999	39.362087
2773.380676	265360.035470	39.367104
2776.503950	265728.851829	39.372122
2779.657790	266105.310015	39.377140
2782.001077	266479.153337	39.382157
2785.078686	266844.853247	39.387175
2787.974642	267223.563248	39.392192
2790.651980	267586.126279	39.397210
2793.482786	267959.182201	39.402228
2796.358060	268331.951890	39.407245
2799.139445	268687.411631	39.412263
2801.710777	269027.485029	39.417280
2804.339775	269364.170826	39.422298
2807.278309	269702.204950	39.427316
2809.773498	270048.311485	39.432333
2812.430088	270372.875972	39.437351
2815.101572	270726.931527	39.442368
2817.464452	271075.853797	39.447386
2820.275379	271427.956872	39.452404
2822.800296	271791.409856	39.457421
2825.396544	272153.327450	39.462439
2828.107784	272529.605255	39.467456
2830.827773	272906.491446	39.472474
2833.559135	273283.147283	39.477492
2835.949660	273663.362825	39.482509
2838.773082	274064.797935	39.487527
2841.704974	274471.093368	39.492544
2844.388287	274874.557601	39.497562
2847.395988	275273.296250	39.502580
2850.102885	275675.664405	39.507597
2853.311913	276083.389363	39.512615
2856.207688	276499.191360	39.517632
2859.257329	276905.595078	39.522650
2862.322744	277318.905952	39.527668
2865.088331	277732.442032	39.532685
2867.913054	278146.679933	39.537703
2870.999558	278550.283049	39.542720
2874.016055	278964.845966	39.547738
2877.073077	279376.379304	39.552756
2879.539061	279802.663777	39.557773
2882.722211	280211.255385	39.562791
2885.331388	280642.546617	39.567808
2888.745274	281071.423894	39.572826
2891.969594	281473.123991	39.577844
2894.574231	281904.694584	39.582861
2897.743049	282309.883176	39.587879
2900.645730	282736.198301	39.592896
2903.121013	283154.121480	39.597914
2906.425613	283578.238414	39.602932
2909.687386	283999.694423	39.607949
2912.707616	284413.135488	39.612967
2915.541521	284837.020943	39.617984
2918.921583	285249.438918	39.623002
2921.954780	285668.008121	39.628020
2924.542760	286101.330311	39.633037
2927.391337	286503.390440	39.638055
2930.334784	286926.011514	39.643072
2932.951757	287345.127341	39.648090
2936.162693	287769.432420	39.653108
2938.759608	288197.187325	39.658125
2941.859041	288618.917824	39.663143
2944.556985	289055.495728	39.668160
2947.441798	289488.588622	39.673178
2950.584638	289906.931827	39.678196
2953.707991	290343.008562	39.683213
2956.520758	290760.208777	39.688231
2959.440723	291154.249577	39.693248
2962.087989	291542.185512	39.698266
2964.930918	291926.508110	39.703284
2967.803886	292332.493671	39.708301
2970.602402	292728.507159	39.713319
2973.246052	293131.682560	39.718336
2976.255630	293540.997494	39.723354
2979.396300	293952.424716	39.728372
2981.812647	294378.013256	39.733389
2984.448892	294784.616088	39.738407
2987.501934	295209.365494	39.743424
2990.004531	295642.456823	39.748442
2993.361536	296080.263757	39.753460
2996.367461	296529.073533	39.758477
2999.268279	296967.941333	39.763495
3001.953361	297415.859909	39.768512
3004.965229	297877.925270	39.773530
3008.509526	298322.276365	39.778548
3011.327151	298786.656260	39.783565
3014.192736	299243.686251	39.788583
3017.659216	299712.888837	39.793600
3020.250393	300173.871554	39.798618
3023.412222	300641.443210	39.803636
3026.222285	301114.657459	39.808653
3029.659186	301584.646720	39.813671
3032.922417	302060.758310	39.818688
3035.396964	302538.999910	39.823706
3038.734314	303018.449670	39.828724
3041.986759	303498.089102	39.833741
3045.040710	303978.774380	39.838759
3048.350338	304452.940372	39.843776
3051.472237	304943.822678	39.848794
3054.673305	305411.474590	39.853812
3057.623867	305892.448964	39.858829
3061.032985	306370.072374	39.863847
3064.215837	306855.654729	39.868864
3067.005180	307330.299247	39.873882
3070.751809	307812.004114	39.878900
3073.639166	308290.820505	39.883917
3076.527058	308777.712109	39.888935
3079.849429	309250.766318	39.893952
3082.937978	309736.276099	39.898970
3086.110978	310206.886365	39.903988
3088.938189	310699.570784	39.909005
3092.287503	311180.613756	39.914023
3095.486116	311656.700276	39.919040
3098.399006	312135.979473	39.924058
3101.820806	312618.020744	39.929076
3104.564939	313109.107530	39.934093
3107.745812	313589.328471	39.939111
3110.815243	314075.355769	39.944128
3114.177821	314559.150147	39.949146
3117.160993	315052.475915	39.954164
3120.169685	315537.997978	39.959181
3123.307569	316008.639315	39.964199
3126.287319	316462.921691	39.969216
3128.948166	316926.624283	39.974234
3132.000997	317366.414070	39.979252
3134.900625	317823.775924	39.984269
3138.010802	318277.952970	39.989287
3140.787576	318732.104393	39.994304
3143.522284	319214.933878	39.999322
3146.874809	319683.897795	40.004340
3149.852075	320167.902964	40.009357
3153.112339	320636.292437	40.014375
3156.429654	321120.695826	40.019392
3159.406746	321610.331319	40.024410
3162.321493	322094.716859	40.029428
3165.812412	322592.062279	40.034445
3168.366420	323100.270264	40.039463
3171.550323	323602.839205	40.044480
3174.903233	324109.390959	40.049498
3178.348788	324615.721806	40.054516
3180.994355	325140.689510	40.059533
3184.356617	325648.525492	40.064551
3187.756344	326166.916790	40.069568
3190.781236	326707.711730	40.074586
3194.292687	327224.123030	40.079604
3197.557704	327748.594657	40.084621
3200.550311	328275.873841	40.089639
3204.277000	328798.157535	40.094656
3207.301179	329336.877278	40.099674
3210.547389	329855.191992	40.104692
3213.888437	330398.881985	40.109709
3217.418156	330936.951509	40.114727
3220.804425	331462.647724	40.119744
3224.228076	331994.022312	40.124762
3227.512682	332526.430681	40.129780
3230.871742	333053.566939	40.134797
3234.031584	333597.515372	40.139815
3236.952203	334118.999596	40.144832
3240.327915	334652.697798	40.149850
3243.833999	335191.271904	40.154868
3247.112300	335728.989047	40.159885
3250.460210	336268.163601	40.164903
3254.020749	336795.645435	40.169920
3257.243675	337341.026580	40.174938
3260.410917	337869.755406	40.179956
3264.023144	338398.511103	40.184973
3267.188784	338925.530357	40.189991
3270.609501	339465.784152	40.195008
3273.781383	340000.563003	40.200026
3277.258083	340534.806675	40.205044
3280.426401	341065.819251	40.210061
3283.639365	341594.027340	40.215079
3287.273999	342124.398451	40.220096
3290.290312	342672.457445	40.225114
3293.558303	343196.225192	40.230132
3296.905005	343733.457328	40.235149
3300.016915	344243.860689	40.240167
3303.314733	344752.986200	40.245184
3306.232091	345237.896446	40.250202
3309.369130	345728.175518	40.255220
3312.582398	346238.824652	40.260237
3315.726634	346742.320899	40.265255
3319.057520	347240.934213	40.270272
3321.625539	347754.769026	40.275290
3325.072883	348269.500918	40.280308
3328.047202	348789.557868	40.285325
3331.310566	349314.286057	40.290343
3334.511165	349847.498085	40.295360
3337.460755	350397.194564	40.300378
3340.913750	350937.337056	40.305396
3344.528937	351490.242626	40.310413
3347.519961	352047.302769	40.315431
3350.948511	352601.013231	40.320448
3354.128097	353168.084059	40.325466
3357.752931	353739.012855	40.330484
3361.011467	354294.864497	40.335501
3364.562152	354866.528681	40.340519
3368.302240	355439.958727	40.345536
3371.206302	356024.023063	40.350554
3374.943486	356587.693463	40.355572
3378.210794	357173.692205	40.360589
3381.523261	357760.565260	40.365607
3385.253464	358342.821922	40.370624
3388.593915	358930.971036	40.375642
3392.171692	359512.451004	40.380660
3395.721286	360110.375248	40.385677
3398.925755	360694.311136	40.390695
3402.641686	361273.818955	40.395712
3405.639539	361879.270013	40.400730
3409.569839	362466.977736	40.405748
3413.010932	363071.556504	40.410765
3416.156100	363659.855483	40.415783
3419.954313	364255.098944	40.420800
3422.910917	364863.309146	40.425818
3425.663084	365488.902048	40.430836
3429.863437	366079.134660	40.435853
3433.092457	366698.925338	40.440871
3437.650194	367290.278144	40.445888
3440.870364	367894.218289	40.450906
3444.404495	368503.835509	40.455924
3448.239772	369109.640959	40.460941
3451.489939	369703.781572	40.465959
3455.447762	370297.878222	40.470976
3458.750347	370887.122120	40.475994
3462.240691	371481.428432	40.481012
3466.254099	372076.125792	40.486029
3469.573438	372658.034585	40.491047
3473.068881	373240.668622	40.496064
3476.365355	373837.991550	40.501082
3480.100879	374421.484419	40.506100
3483.887352	374996.537311	40.511117
3487.051595	375564.974922	40.516122
3490.738788	376091.135227	40.521127
3493.899740	376568.737816	40.526132
3496.794370	376992.554370	40.531136
3499.553063	377368.797716	40.536141
3502.227418	377677.951993	40.541146
3504.208937	377942.854162	40.546151
3505.992831	378170.930207	40.551156
3507.747905	378344.909091	40.556160
3509.860025	378484.620704	40.561165
3511.015193	378580.124590	40.566170
3512.275363	378649.057626	40.571175
3513.339986	378685.541138	40.576180
3514.250161	378695.444174	40.581184
3515.171085	378679.605425	40.586189
3515.804575	378630.441527	40.591194
3516.444187	378563.802794	40.596199
3516.535898	378495.648157	40.601204
3516.914865	378391.686315	40.606208
3517.468170	378287.340549	40.611213
3517.413470	378169.686272	40.616218
3517.733894	378045.893312	40.621223
3517.700604	377914.728755	40.626228
3517.930291	377765.615631	40.631232
3517.800599	377615.821127	40.636237
3517.228473	377463.094591	40.641242
3517.260689	377290.101376	40.646247
3516.819875	377142.236517	40.651252
3516.776202	376989.577242	40.656256
3516.861122	376835.167405	40.661261
3516.405047	376678.248005	40.666266
3516.667273	376509.488327	40.671271
3516.162633	376349.802767	40.676276
3516.150852	376196.779323	40.681280
3515.869751	376035.988850	40.686285
3515.463159	375879.821608	40.691290
3515.029211	375717.782197	40.696295
3514.773666	375577.589630	40.701300
3514.763112	375432.804638	40.706304
3514.421243	375281.432439	40.711309
3513.852825	375145.205142	40.716314
3513.828074	374994.799230	40.721319
3513.394582	374872.463844	40.726324
3513.352317	374723.357002	40.731328
3512.859501	374598.155749	40.736333
3512.192670	374467.817800	40.741338
3512.419108	374348.225527	40.746343
3512.128112	374239.042404	40.751348
3511.764948	374116.795394	40.756352
3511.640079	374008.297653	40.761357
3511.241760	373897.044686	40.766362
3511.311059	373791.542790	40.771367
3511.205288	373691.969921	40.776372
3511.117135	373583.999459	40.781376
3510.700495	373485.365568	40.786381
3510.297241	373385.381102	40.791386
3510.398661	373282.950853	40.796391
3510.001238	373205.681403	40.801396
3509.589353	373119.408911	40.806400
3509.594325	373021.775679	40.811405
3509.102489	372943.070675	40.816410
3509.296948	372863.722819	40.821415
3509.194179	372786.736711	40.826420
3509.396065	372717.588271	40.831424
3509.302032	372645.662806	40.836429
3508.680872	372576.771437	40.841434
3508.961881	372489.955649	40.846439
3508.708147	372422.761216	40.851444
3508.523081	372346.168887	40.856448
3508.775223	372277.851258	40.861453
3508.141869	372216.084110	40.866458
3508.192981	372152.020916	40.871463
3507.786619	372097.773081	40.876468
3507.704730	372032.687732	40.881472
3507.529926	371982.193558	40.886477
3507.492226	371934.704901	40.891482
3507.746386	371872.160967	40.896487
3507.440929	371808.255374	40.901492
3507.412604	371764.860750	40.906496
3507.239359	371718.945069	40.911501
3507.335320	371663.904966	40.916506
3507.354935	371614.753336	40.921511
3507.237904	371564.427602	40.926516
3507.389055	371522.301761	40.931520
3507.253004	371461.675977	40.936525
3506.578688	371417.187466	40.941530
3507.079331	371370.478010	40.946535
3506.793711	371323.841920	40.951540
3506.704555	371288.698808	40.956544
3506.736323	371241.325587	40.961549
3506.745873	371192.912804	40.966554
3506.332902	371151.842476	40.971559
3506.146736	371121.090166	40.976564
3506.586305	371087.415118	40.981568
3506.266624	371049.484454	40.986573
3505.969705	371019.970681	40.991578
3506.081475	370977.570688	40.996583
3506.217156	370959.512654	41.001588
3505.858537	370926.319816	41.006592
3505.956561	370897.175997	41.011597
3505.853988	370860.279311	41.016602
3506.092485	370820.199583	41.021607
3505.585773	370805.702845	41.026612
3505.511826	370767.707643	41.031616
3505.841516	370742.775541	41.036621
3505.749356	370721.649768	41.041626
3505.544199	370684.972665	41.046631
3505.784836	370662.471380	41.051636
3505.452240	370635.278007	41.056640
3505.403037	370609.006532	41.061645
3505.568115	370594.988638	41.066650
3505.494978	370567.754205	41.071655
3505.524131	370545.795090	41.076660
3505.734110	370514.852517	41.081664
3505.729835	370488.650185	41.086669
3505.548823	370472.804406	41.091674
3505.686398	370433.579789	41.096679
3505.503227	370419.744091	41.101684
3505.467915	370390.722766	41.106688
3505.260092	370370.073023	41.111693
3505.651247	370339.712243	41.116698
3505.781275	370319.492428	41.121703
3505.400216	370296.326029	41.126708
3505.194600	370261.607521	41.131712
3505.732290	370245.826122	41.136717
3505.225308	370222.908552	41.141722
3505.334274	370200.529600	41.146727
3505.424321	370170.852304	41.151732
3505.364132	370155.546990	41.156736
3505.520035	370128.301510	41.161741
3505.235677	370121.401439	41.166746
3505.425004	370092.726002	41.171751
3505.161383	370077.122098	41.176756
3505.122212	370050.161808	41.181760
3505.415980	370019.714436	41.186765
3505.155916	370015.125569	41.191770
3505.396229	369984.279579	41.196775
3505.428391	369963.439060	41.201780
3505.204065	369941.926751	41.206784
3505.172888	369924.937710	41.211789
3504.839762	369901.076632	41.216794
3505.213471	369880.741766	41.221799
3504.881013	369875.426560	41.226804
3504.866272	369846.783219	41.231808
3505.082340	369839.422387	41.236813
3504.967978	369814.712587	41.241818
3505.090848	369790.194232	41.246823
3504.899125	369777.962423	41.251828
3504.816262	369756.631180	41.256832
3505.072730	369732.854885	41.261837
3504.894696	369724.487839	41.266842
3505.127439	369701.325847	41.271847
3504.941610	369695.936557	41.276852
3504.702332	369660.485112	41.281856
3504.803547	369654.897797	41.286861
3504.578971	369640.076215	41.291866
3504.707191	369624.486523	41.296871
3505.193774	369617.362734	41.301876
3504.865491	369600.674938	41.306880
3504.758048	369587.564774	41.311885
3504.887871	369561.976690	41.316890
3505.169467	369543.030015	41.321895
3504.726439	369533.000308	41.326900
3504.656149	369519.121034	41.331904
3504.667054	369491.999835	41.336909
3504.499497	369484.165337	41.341914
3504.755399	369463.136563	41.346919
3504.506521	369460.530233	41.351924
3504.371521	369441.852896	41.356928
3504.436130	369431.157782	41.361933
3504.357245	369429.669403	41.366938
3504.993108	369412.142219	41.371943
3504.719279	369408.852935	41.376948
3504.660061	369392.707656	41.381952
3504.936928	369379.663878	41.386957
3504.790946	369361.853224	41.391962
3504.794258	369343.713673	41.396967
3504.887979	369334.336846	41.401972
3504.675410	369310.787111	41.406976
3504.958249	369299.421448	41.411981
3504.570087	369281.343758	41.416986
3504.600610	369258.569666	41.421991
3504.498196	369246.043740	41.426996
3504.254880	369243.843568	41.432000
3504.391963	369243.847483	41.437005
3504.664295	369234.518720	41.442010
3504.330772	369223.250476	41.447015
3504.334376	369212.870240	41.452020
3504.436806	369201.024258	41.457024
3504.609037	369191.940277	41.462029
3504.252417	369182.227558	41.467034
3504.336304	369161.251271	41.472039
3504.299142	369157.746468	41.477044
3504.609067	369146.351042	41.482048
3504.429203	369128.138596	41.487053
3504.244958	369122.876188	41.492058
3504.499701	369116.221461	41.497063
3504.378804	369111.508734	41.502068
3504.465042	369086.970331	41.507072
3504.797862	369093.252618	41.512077
3504.237848	369079.399740	41.517082
3504.702430	369067.750878	41.522087
3504.393687	369058.056003	41.527092
3504.318637	369040.030476	41.532096
3504.432701	369045.889418	41.537101
3504.393101	369027.781959	41.542106
3504.385085	369009.771263	41.547111
3504.133652	369014.823001	41.552116
3504.341698	368993.114662	41.557120
3504.480155	368975.894904	41.562125
3503.922305	368981.478462	41.567130
3504.714701	368961.484029	41.572135
3504.346339	368960.728300	41.577140
3504.324862	368942.923231	41.582144
3504.257652	368935.734233	41.587149
3504.484280	368931.297279	41.592154
3504.533991	368912.259782	41.597159
3504.209177	368914.295665	41.602164
3504.462939	368907.234007	41.607168
3504.447877	368889.173493	41.612173
3504.089767	368890.553178	41.617178
3504.136895	368871.643276	41.622183
3504.463480	368865.918467	41.627188
3504.209374	368859.878403	41.632192
3504.293278	368857.804569	41.637197
3504.005102	368842.814682	41.642202
3504.857455	368831.664155	41.647207
3504.213219	368823.650485	41.652212
3504.493786	368806.891572	41.657216
3504.635188	368799.720455	41.662221
3504.144234	368793.539737	41.667226
3504.591697	368777.543098	41.672231
3504.396529	368777.472333	41.677236
3504.301178	368764.970592	41.682240
3504.341229	368764.353822	41.687245
3504.044883	368751.018858	41.692250
3504.128159	368735.385069	41.697255
3504.144203	368741.488517	41.702260
3504.172658	368728.789106	41.707264
3504.069061	368713.006764	41.712269
3504.092014	368726.308927	41.717274
3504.383251	368711.049310	41.722279
3504.502080	368700.854264	41.727284
3504.421086	368685.526277	41.732288
3504.466787	368681.397751	41.737293
3504.295197	368667.686865	41.742298
3504.585799	368646.448682	41.747303
3504.389765	368636.964864	41.752308
3504.128052	368636.141387	41.757312
3504.572743	368624.342904	41.762317
3504.053172	368614.833905	41.767322
3504.399753	368601.524463	41.772327
3504.212076	368599.569873	41.777332
3504.399936	368583.207146	41.782336
3504.544956	368575.602922	41.787341
3504.129344	368563.787779	41.792346
3504.448423	368541.044018	41.797351
3504.133427	368551.550254	41.802356
3504.205700	368546.908693	41.807360
3504.559724	368521.691610	41.812365
3504.268496	368526.469842	41.817370
3504.245982	368506.451382	41.822375
3504.432160	368486.959626	41.827380
3504.583208	368479.685166	41.832384
3504.390123	368470.149964	41.837389
3504.249210	368461.064452	41.842394
3504.648272	368452.784016	41.847399
3504.261638	368445.645434	41.852404
3504.119314	368432.387788	41.857408
3503.943553	368435.723071	41.862413
3503.956821	368412.595088	41.867418
3504.042790	368407.391640	41.872423
3504.041840	368407.697230	41.877428
3503.963228	368414.629805	41.882432
3504.245701	368393.087489	41.887437
3504.040956	368383.554111	41.892442
3504.451528	368375.500812	41.897447
3504.484707	368376.462477	41.902452
3504.300358	368368.833962	41.907456
3504.640404	368375.522271	41.912461
3504.148061	368358.198460	41.917466
3504.337815	368349.060651	41.922471
3504.541844	368337.223813	41.927476
3504.252491	368318.341423	41.932480
3504.339236	368317.640941	41.937485
3504.085721	368313.228946	41.942490
3504.251765	368286.387764	41.947495
3504.137545	368285.439198	41.952500
3503.862399	368282.887832	41.957504
3504.254773	368266.441773	41.962509
3504.314821	368261.395053	41.967514
3504.115067	368256.287639	41.972519
3504.291213	368256.412586	41.977524
3504.294502	368226.951204	41.982528
3504.438550	368226.496075	41.987533
3503.823161	368223.362460	41.992538
3504.318525	368202.295221	41.997543
3504.128171	368199.348826	42.002548
3504.089089	368196.861901	42.007552
3504.413453	368185.667473	42.012557
3504.185571	368172.703128	42.017562
3504.240487	368171.015464	42.022567
3504.132821	368159.507708	42.027572
3504.121107	368147.730367	42.032576
3504.163385	368145.001605	42.037581
3503.862308	368150.824530	42.042586
3504.317611	368119.790580	42.047591
3504.559513	368121.864116	42.052596
3504.099815	368111.862155	42.057600
3504.507082	368086.102136	42.062605
3504.095925	368085.836542	42.067610
3504.301505	368073.541443	42.072615
3503.921408	368065.333227	42.077620
3504.130464	368054.080670	42.082624
3504.167328	368054.507491	42.087629
3503.841072	368052.422135	42.092634
3504.003454	368034.282334	42.097639
3503.995579	368033.724013	42.102644
3503.948440	368027.040520	42.107648
3504.135749	368026.654874	42.112653
3503.891458	368023.411696	42.117658
3503.940533	368007.859378	42.122663
3503.641774	368016.480511	42.127668
3503.869136	368008.405225	42.132672
3503.922202	368010.152439	42.137677
3503.779707	368016.713555	42.142682
3504.265747	367988.320559	42.147687
3504.193425	367983.829004	42.152692
3504.137598	367985.262695	42.157696
3504.288762	367980.964782	42.162701
3503.973768	367969.387986	42.167706
3504.096472	367950.796476	42.172711
3503.421704	367965.710217	42.177716
3503.961999	367959.213704	42.182720
3503.924743	367957.744134	42.187725
3503.730364	367953.958791	42.192730
3503.868641	367954.674878	42.197735
3503.878623	367954.190057	42.202740
3503.900122	367949.505576	42.207744
3504.150988	367951.246965	42.212749
3503.796088	367931.993148	42.217754
3503.914419	367927.598654	42.222759
3504.045681	367928.850122	42.227764
3504.162525	367928.602822	42.232768
3504.297072	367913.520347	42.237773
3503.806524	367903.574099	42.242778
3503.991089	367902.298434	42.247783
3504.041917	367908.065760	42.252788
3504.006916	367889.931660	42.257792
3504.200200	367881.123935	42.262797
3504.105551	367874.498813	42.267802
3504.147721	367870.040029	42.272807
3503.699041	367868.584615	42.277812
3503.693749	367858.434436	42.282816
3504.217417	367852.525691	42.287821
3503.779826	367858.243028	42.292826
3503.807182	367848.469309	42.297831
3503.940123	367856.640604	42.302836
3504.177736	367844.391260	42.307840
3504.060941	367829.679229	42.312845
3503.979851	367832.796060	42.317850
3504.303872	367826.537249	42.322855
3503.837388	367811.676962	42.327860
3504.168176	367801.473640	42.332864
3504.087442	367803.420105	42.337869
3504.044044	367804.317565	42.342874
3504.095098	367786.398793	42.347879
3503.959213	367774.742747	42.352884
3503.777136	367775.662131	42.357888
3503.899514	367784.064083	42.362893
3503.903290	367772.793023	42.367898
3504.208933	367757.785212	42.372903
3503.769885	367758.770662	42.377908
3503.594793	367755.414758	42.382912
3504.003538	367755.172195	42.387917
3503.980460	367747.365427	42.392922
3504.143957	367726.274099	42.397927
3503.976186	367730.753044	42.402932
3504.084002	367736.613149	42.407936
3504.024702	367717.439715	42.412941
3504.020182	367718.738096	42.417946
3504.246232	367694.354899	42.422951
3504.021310	367701.514250	42.427956
3504.046735	367688.357068	42.432960
3503.870202	367677.089046	42.437965
3503.793192	367680.332450	42.442970
3503.955980	367676.719593	42.447975
3503.811639	367682.924868	42.452980
3503.926511	367664.843308	42.457984
3503.733737	367650.423086	42.462989
3503.515069	367656.309374	42.467994
3503.976284	367644.075509	42.472999
3503.859002	367652.184632	42.478004
3503.951926	367654.739691	42.483008
3504.179534	367650.709519	42.488013
3503.838660	367628.502123	42.493018
3504.216977	367614.424115	42.498023
3503.824388	367625.146373	42.503028
3503.908331	367621.749509	42.508032
3503.947106	367610.447433	42.513037
3503.554441	367601.096242	42.518042
3504.032190	367590.309923	42.523047
3503.779318	367600.068757	42.528052
3504.031308	367612.724451	42.533056
3503.852864	367600.566254	42.538061
3503.773615	367586.382481	42.543066
3504.118411	367582.715402	42.548071
3504.107550	367586.050122	42.553076
3503.946540	367575.237570	42.558080
3504.359310	367570.160453	42.563085
3503.901851	367565.602531	42.568090
3504.215188	367550.924176	42.573095
3504.241989	367567.228201	42.578100
3504.025262	367543.042126	42.583104
3503.929170	367529.140856	42.588109
3504.020374	367532.408562	42.593114
3503.993406	367526.077987	42.598119
3504.010180	367514.041556	42.603124
3504.183181	367510.096328	42.608128
3504.314165	367504.198732	42.613133
3503.771292	367497.822503	42.618138
3504.221603	367478.135893	42.623143
3504.205191	367476.001527	42.628148
3504.024708	367480.813249	42.633152
3504.181045	367471.833191	42.638157
3504.080509	367460.247799	42.643162
3503.722866	367443.258516	42.648167
3503.716922	367449.238411	42.653172
3503.847408	367445.986826	42.658176
3504.229708	367437.861501	42.663181
3503.838980	367430.621632	42.668186
3503.680917	367417.238959	42.673191
3504.143078	367418.081945	42.678196
3503.644112	367422.155327	42.683200
3503.913909	367419.187018	42.688205
3503.692977	367405.788838	42.693210
3504.094296	367395.345297	42.698215
3503.894788	367403.747325	42.703220
3503.494358	367394.804385	42.708224
3503.893423	367401.025561	42.713229
3503.785041	367405.113523	42.718234
3504.098164	367371.201161	42.723239
3503.970733	367370.712615	42.728244
3503.918945	367364.131523	42.733248
3504.050865	367373.218974	42.738253
3504.056025	367355.434491	42.743258
3503.836239	367336.515239	42.748263
3503.754960	367340.548038	42.753268
3503.658142	367344.150783	42.758272
3504.161825	367349.592174	42.763277
3503.924319	367342.378952	42.768282
3503.969647	367323.672201	42.773287
3504.241549	367316.251234	42.778292
3503.908500	367316.889192	42.783296
3503.838812	367312.193617	42.788301
3503.706526	367297.611067	42.793306
3504.170971	367285.529243	42.798311
3503.984504	367281.742590	42.803316
3503.894648	367285.522333	42.808321
3504.178772	367282.297332	42.813325
3503.875937	367271.227266	42.818330
3504.094856	367250.076066	42.823335
3504.253318	367261.220134	42.828340
3503.885146	367253.874903	42.833345
3503.873275	367240.443623	42.838349
3503.905238	367238.199831	42.843354
3504.074216	367229.624796	42.848359
3503.744549	367233.340686	42.853364
3503.915726	367237.206376	42.858369
3504.013383	367211.138605	42.863373
3503.778611	367209.878328	42.868378
3503.759371	367210.135934	42.873383
3503.995599	367213.864132	42.878388
3503.772579	367208.047902	42.883393
3504.124313	367196.390942	42.888397
3503.924372	367182.734957	42.893402
3504.051909	367176.379908	42.898407
3504.030613	367181.013845	42.903412
3503.819952	367178.553987	42.908417
3504.018791	367155.650425	42.913421
3503.963302	367152.784406	42.918426
3504.133838	367142.479057	42.923431
3504.232492	367154.650284	42.928436
3504.232134	367137.655285	42.933441
3504.263322	367134.063188	42.938445
3503.998017	367129.220425	42.943450
3504.466098	367110.370426	42.948455
3503.993073	367091.541986	42.953460
3503.824273	367086.226007	42.958465
3504.139956	367078.085705	42.963469
3503.902178	367081.380010	42.968474
3503.952449	367076.003955	42.973479
3503.812290	367066.409196	42.978484
3503.978279	367059.208466	42.983489
3504.027368	367047.421218	42.988493
3503.525575	367047.577016	42.993498
3503.854256	367032.361782	42.998503
3503.719494	367029.101215	43.003508
3503.673628	367033.739052	43.008513
3503.963444	367025.043106	43.013517
3503.915965	367035.278435	43.018522
3504.072187	367035.304767	43.023527
3504.061787	367014.596779	43.028532
3503.440983	367009.581224	43.033537
3503.708435	366999.438615	43.038541
3503.545410	367013.762935	43.043546
3503.791653	367010.518461	43.048551
3503.580189	367014.953500	43.053556
3503.571156	367012.996040	43.058561
3504.011177	367001.325073	43.063565
3503.860986	366995.573626	43.068570
3503.729153	366983.458775	43.073575
3503.519929	366992.702003	43.078580
3503.636050	366984.084392	43.083585
3503.669260	366991.940867	43.088589
3503.524966	366998.705955	43.093594
3504.022838	366987.712772	43.098599
3503.930829	366989.075889	43.103604
3503.765407	366981.164278	43.108609
3503.885092	366975.980774	43.113613
3503.753074	366970.455430	43.118618
3504.021496	366972.092314	43.123623
3503.797011	366978.590219	43.128628
3503.630428	366960.451097	43.133633
3504.006947	366939.631023	43.138637
3503.807675	366941.367286	43.143642
3504.070512	366937.585901	43.148647
3503.896085	366940.793875	43.153652
3503.931529	366938.956591	43.158657
3504.211482	366914.920632	43.163661
3504.165152	366915.844015	43.168666
3504.150113	366912.259208	43.173671
3503.692785	366899.305318	43.178676
3503.930719	366879.626575	43.183681
3503.888534	366868.591529	43.188685
3503.959184	366887.229544	43.193690
3503.815451	366876.108785	43.198695
3504.102308	366878.836767	43.203700
3503.957518	366869.319024	43.208705
3503.970600	366855.934567	43.213709
3503.921151	366845.180526	43.218714
3503.726618	366842.260142	43.223719
3503.892542	366850.299199	43.228724
3504.117862	366831.436575	43.233729
3503.605158	366819.102027	43.238733
3503.618149	366832.355453	43.243738
3503.781182	366820.168500	43.248743
3503.782942	366824.569851	43.253748
3503.436374	366830.552793	43.258753
3504.125353	366821.488400	43.263757
3503.955572	366806.301004	43.268762
3503.650767	366796.325142	43.273767
3503.717127	366810.104422	43.278772
3503.414495	366805.038545	43.283777
3503.857538	366804.561577	43.288781
3503.438466	366805.569330	43.293786
3503.921825	366801.422324	43.298791
3503.831320	366808.077168	43.303796
3503.657849	366788.387096	43.308801
3503.570862	366782.142230	43.313805
3503.632438	366781.089514	43.318810
3503.638773	366777.297780	43.323815
3503.918237	366788.702702	43.328820
3503.883457	366785.375427	43.333825
3503.855304	366785.888866	43.338829
3503.380602	366785.378886	43.343834
3503.766004	366770.027385	43.348839
3503.586685	366766.137789	43.353844
3503.780937	366769.109397	43.358849
3503.786161	366767.633073	43.363853
3503.625505	366765.750455	43.368858
3503.883945	366761.689887	43.373863
3503.590074	366772.371301	43.378868
3503.590434	366770.692209	43.383873
3503.879558	366763.675502	43.388877
3503.735628	366745.914343	43.393882
3503.698048	366739.890640	43.398887
3503.812143	366745.699000	43.403892
3503.857796	366737.855746	43.408897
3504.003727	366737.069557	43.413901
3504.044960	366739.709167	43.418906
3504.061643	366722.762199	43.423911
3503.598195	366723.497106	43.428916
3503.841408	366726.104787	43.433921
3503.999755	366717.862081	43.438925
3503.746186	366730.572508	43.443930
3504.081070	366704.695916	43.448935
3503.912626	366695.054664	43.453940
3503.877692	366692.592441	43.458945
3503.986357	366692.117448	43.463949
3503.883867	366687.910394	43.468954
3504.060905	366663.966895	43.473959
3503.798010	366660.523020	43.478964
3503.688524	366662.499523	43.483969
3504.099030	366659.585246	43.488973
3503.937218	366668.286759	43.493978
3503.723485	366648.399453	43.498983
3503.542166	366632.399671	43.503988
3503.699243	366637.437984	43.508993
3503.789067	366630.808955	43.513997
3503.862793	366634.690103	43.519002
3503.848970	366631.155966	43.524007
3503.651025	366637.191765	43.529012
3503.738038	366629.774471	43.534017
3504.006588	366616.705747	43.539021
3503.942012	366609.312413	43.544026
3503.928448	366600.969652	43.549031
3503.818928	366602.997047	43.554036
3503.790566	366608.242774	43.559041
3503.909744	366594.994120	43.564045
3503.511146	366586.432360	43.569050
3503.489069	366578.370805	43.574055
3503.629212	366581.936151	43.579060
3503.276768	366577.895813	43.584065
3503.565128	366579.605886	43.589069
3503.541310	366585.537839	43.594074
3503.683338	366585.617300	43.599079
3503.608555	366593.058400	43.604084
3503.685015	366593.428092	43.609089
3503.889847	366586.679105	43.614093
3503.789248	366584.023718	43.619098
3503.909373	366558.613511	43.624103
3504.002387	366559.769295	43.629108
3503.737191	366562.966204	43.634113
3504.118085	366562.015655	43.639117
3503.722224	366555.616048	43.644122
3503.868706	366542.006870	43.649127
3503.654325	366543.923633	43.654132
3503.520010	366531.783609	43.659137
3503.549556	366536.358691	43.664141
3503.434713	366536.987606	43.669146
3503.691279	366531.349892	43.674151
3503.622112	366535.329966	43.679156
3503.566757	366548.034551	43.684161
3503.823101	366546.518520	43.689165
3503.575995	366543.759081	43.694170
3503.805354	366542.120105	43.699175
3503.761490	366530.474626	43.704180
3503.788819	366516.324546	43.709185
3504.030138	366514.861774	43.714189
3503.707596	366516.617542	43.719194
3503.802444	366511.208929	43.724199
3503.574373	366528.189686	43.729204
3503.474446	366518.206814	43.734209
3503.617280	366510.755233	43.739213
3503.649002	366494.365531	43.744218
3503.679610	366484.082151	43.749223
3503.401884	366491.122832	43.754228
3503.800033	366490.525746	43.759233
3504.045140	366484.584531	43.764237
3503.560309	366500.053908	43.769242
3503.604897	366491.930914	43.774247
3503.915168	366495.774680	43.779252
3503.674507	366490.190124	43.784257
3503.835313	366473.805450	43.789261
3503.597826	366466.566640	43.794266
3503.708569	366469.882220	43.799271
3503.768371	366467.099699	43.804276
3504.041786	366469.371871	43.809281
3504.085747	366463.462451	43.814285
3503.819480	366458.187247	43.819290
3503.616901	366442.852258	43.824295
3503.816863	366446.637140	43.829300
3503.555530	366437.672017	43.834305
3503.958764	366442.620553	43.839309
3503.888751	366439.680457	43.844314
3503.841713	366439.153750	43.849319
3503.958935	366423.819082	43.854324
3503.925533	366415.250442	43.859329
3504.342726	366414.192383	43.864333
3503.778551	366411.075982	43.869338
3504.061012	366381.976314	43.874343
3504.019586	366381.779469	43.879348
3503.838366	366387.710889	43.884353
3503.907602	366387.038587	43.889357
3504.068586	366381.110657	43.894362
3503.946654	366352.100341	43.899367
3503.510831	366355.146141	43.904372
3503.591376	366351.851487	43.909377
3503.867555	366344.887646	43.914381
3504.046062	366360.990035	43.919386
3503.984207	366349.474565	43.924391
3503.825886	366328.280794	43.929396
3503.853880	366323.849538	43.934401
3503.966777	366316.962391	43.939405
3503.936716	366312.794735	43.944410
3504.124312	366308.185593	43.949415
3503.891886	366298.325388	43.954420
3504.077605	366292.775171	43.959425
3503.913896	366291.732616	43.964429
3503.754947	366297.991278	43.969434
3503.947026	366292.898019	43.974439
3503.965036	366267.631001	43.979444
3503.710935	366255.280856	43.984449
3503.700890	366264.950710	43.989453
3503.539213	366273.448740	43.994458
3503.876776	366263.701959	43.999463
3503.683361	366272.968279	44.004468
3503.516754	366278.210458	44.009473
3503.647636	366259.845928	44.014477
3503.552004	366256.604560	44.019482
3503.426016	366235.634616	44.024487
3503.638370	366236.415349	44.029492
3503.651241	366237.863678	44.034497
3503.747576	366234.617404	44.039501
3503.615206	366242.245764	44.044506
3503.858344	366236.762790	44.049511
3503.845458	366235.594620	44.054516
3503.794208	366243.973429	44.059521
3503.933326	366221.333252	44.064525
3503.444684	366217.339854	44.069530
3503.833067	366214.505373	44.074535
3503.745422	366209.888848	44.079540
3503.857935	366206.105723	44.084545
3503.967574	366207.309773	44.089549
3503.467825	366221.407712	44.094554
3503.727505	366197.171032	44.099559
3503.882174	366188.190979	44.104564
3503.546233	366185.013039	44.109569
3504.095648	366179.201773	44.114573
3503.550252	366181.705173	44.119578
3503.784352	366181.083133	44.124583
3503.640845	366187.288484	44.129588
3503.583006	366191.139585	44.134593
3503.550275	366191.017692	44.139597
3503.312372	366183.778902	44.144602
3503.573176	366164.147112	44.149607
3503.809308	366169.910813	44.154612
3503.514761	366157.643362	44.159617
3503.748699	366165.468251	44.164621
3503.586465	366172.287184	44.169626
3503.582507	366168.318929	44.174631
3503.794884	366170.956960	44.179636
3503.684640	366162.095108	44.184641
3503.882781	366169.900213	44.189645
3503.501070	366165.406499	44.194650
3503.932123	366145.238937	44.199655
3503.970713	366140.526121	44.204660
3503.405700	366138.681958	44.209665
3503.823438	366144.366067	44.214669
3503.646561	366151.289088	44.219674
3503.978031	366150.142805	44.224679
3503.781077	366151.522538	44.229684
3503.644593	366133.836286	44.234689
3503.889687	366117.819794	44.239693
3503.720316	366119.678575	44.244698
3503.778694	366112.113067	44.249703
3503.696039	366118.232480	44.254708
3503.835753	366118.032441	44.259713
3504.079022	366116.136825	44.264717
3503.922227	366093.263496	44.269722
3504.112369	366082.903918	44.274727
3503.891959	366087.645774	44.279732
3503.641276	366087.151256	44.284737
3503.837560	366080.734297	44.289741
3503.392907	366062.460672	44.294746
3503.847075	366049.540535	44.299751
3503.891361	366048.185224	44.304756
3503.758597	366051.361233	44.309761
3504.047878	366049.153030	44.314765
3503.654869	366057.992982	44.319770
3503.906649	366046.987588	44.324775
3503.703711	366033.458937	44.329780
3503.827966	366027.027915	44.334785
3504.127248	366017.236246	44.339789
3503.496489	366024.154713	44.344794
3503.731460	366010.226073	44.349799
3503.697624	366014.302378	44.354804
3503.657555	366012.680533	44.359809
3503.668357	365995.810546	44.364813
3503.461859	365993.986028	44.369818
3503.682566	365990.312994	44.374823
3503.381846	365989.292091	44.379828
3503.527087	365983.239384	44.384833
3503.501231	365987.212659	44.389837
3503.292519	366000.730364	44.394842
3503.467564	365988.006991	44.399847
3503.697798	365993.873417	44.404852
3503.665765	366006.574470	44.409857
3503.654226	366002.734611	44.414861
3503.790900	366000.830399	44.419866
3504.138004	365998.078759	44.424871
3503.784233	365989.738781	44.429876
3503.771889	365977.655651	44.434881
3503.693963	365968.407013	44.439885
3503.444083	365973.636950	44.444890
3503.671124	365969.199635	44.449895
3503.836728	365971.412547	44.454900
3503.848819	365968.993735	44.459905
3504.069419	365966.745501	44.464909
3503.782898	365958.089574	44.469914
3503.864796	365938.231543	44.474919
3503.881401	365945.378435	44.479924
3503.722593	365943.851687	44.484929
3503.667878	365942.969991	44.489933
3503.670925	365946.684274	44.494938
3503.628330	365943.841581	44.499943
3503.813659	365930.047977	44.504948
3503.370225	365917.498687	44.509953
3503.636929	365912.902440	44.514957
3503.503924	365908.242169	44.519962
3503.855172	365902.996490	44.524967
3503.618339	365910.539650	44.529972
3503.359096	365912.921500	44.534977
3503.742681	365912.937333	44.539981
3503.596615	365914.817880	44.544986
3503.727922	365919.784021	44.549991
3503.821093	365925.748451	44.554996
3503.685339	365905.695830	44.560001
3503.746938	365897.035744	44.565005
3503.586321	365888.156359	44.570010
3503.599074	365883.473043	44.575015
3503.672719	365883.690529	44.580020
3503.876224	365882.106501	44.585025
3504.108772	365888.252444	44.590029
3503.605908	365886.881856	44.595034
3503.672203	365875.524103	44.600039
3503.617387	365871.640190	44.605044
3503.302541	365873.725519	44.610049
3503.880277	365864.118782	44.615053
3503.625117	365872.300912	44.620058
3503.718833	365869.869190	44.625063
3503.727707	365874.218624	44.630068
3503.450966	365874.720486	44.635073
3503.868711	365866.512945	44.640077
3503.629571	365878.814249	44.645082
3503.636753	365863.013376	44.650087
3503.617222	365852.356137	44.655092
3503.469742	365850.700382	44.660097
3503.856156	365842.014378	44.665101
3503.701079	365846.822259	44.670106
3504.089263	365840.502143	44.675111
3503.778439	365850.372292	44.680116
3503.603031	365847.499704	44.685121
3503.717549	365842.571311	44.690125
3503.277783	365823.202781	44.695130
3503.674745	365819.985279	44.700135
3503.701560	365814.816322	44.705140
3503.846019	365821.306955	44.710145
3503.582729	365820.356459	44.715149
3503.848281	365819.398687	44.720154
3504.058264	365818.093503	44.725159
3503.917686	365812.289498	44.730164
3503.653977	365793.045778	44.735169
3504.062087	365786.188207	44.740173
3503.926737	365793.282818	44.745178
3504.002177	365785.103933	44.750183
3503.560595	365793.722631	44.755188
3503.886056	365782.120342	44.760193
3503.944700	365762.164138	44.765197
3503.867822	365762.685291	44.770202
3504.107280	365750.791278	44.775207
3503.656425	365758.317412	44.780212
3503.492731	365754.730570	44.785217
3503.712359	365762.786776	44.790221
3503.637198	365744.301952	44.795226
3503.804039	365726.974671	44.800231
3503.499161	365734.146976	44.805236
3503.491608	365732.469095	44.810241
3503.723260	365719.151515	44.815245
3503.456988	365727.767954	44.820250
3503.873436	365725.310648	44.825255
3503.965693	365733.921292	44.830260
3503.963005	365726.136388	44.835265
3503.755221	365706.069622	44.840269
3503.852612	365698.701419	44.845274
3504.175302	365688.142697	44.850279
3503.932455	365689.656912	44.855284
3503.795756	365687.439706	44.860289
3503.820970	365670.185678	44.865293
3503.512834	365672.829697	44.870298
3503.970008	365658.509622	44.875303
3503.896347	365658.572297	44.880308
3503.580988	365663.329208	44.885313
3503.805408	365662.861348	44.890317
3504.034963	365671.017772	44.895322
3504.014805	365640.489783	44.900327
3503.641922	365630.193666	44.905332
3503.737663	365632.264983	44.910337
3503.838301	365628.178374	44.915341
3503.570231	365642.672396	44.920346
3503.594614	365640.556936	44.925351
3503.917337	365648.876735	44.930356
3503.579074	365622.088224	44.935361
3503.740135	365604.685481	44.940365
3503.890841	365598.555530	44.945370
3503.857315	365591.436990	44.950375
3503.681559	365600.446229	44.955380
3503.639371	365608.976380	44.960385
3503.869884	365606.217705	44.965389
3503.500789	365597.752862	44.970394
3503.713667	365584.489096	44.975399
3503.802352	365578.954131	44.980404
3503.568174	365582.476962	44.985409
3504.156747	365574.115147	44.990413
3504.004643	365571.264300	44.995418
3504.095521	365560.513209	45.000423
3503.718430	365555.331747	45.005428
3503.724816	365538.843929	45.010433
3503.904861	365538.103212	45.015437
3503.641387	365540.587521	45.020442
3503.791545	365540.334943	45.025447
3503.913210	365541.613438	45.030452
3503.785962	365532.016308	45.035457
3503.739624	365519.073373	45.040461
3503.478675	365519.623628	45.045466
3503.748039	365506.579894	45.050471
3503.608548	365524.997269	45.055476
3503.700810	365520.352232	45.060481
3504.000051	365515.038401	45.065485
3503.832927	365520.433407	45.070490
3504.125113	365494.893624	45.075495
3503.870203	365487.555638	45.080500
3503.838756	365477.917909	45.085505
3503.626723	365483.218247	45.090509
3503.486750	365479.653076	45.095514
3503.740587	365473.099718	45.100519
3503.709461	365478.117029	45.105524
3503.595323	365459.383821	45.110529
3503.387053	365449.519610	45.115533
3503.221270	365450.360136	45.120538
3503.351522	365446.828572	45.125543
3503.434393	365444.423985	45.130548
3503.680505	365446.420653	45.135553
3503.700351	365451.811552	45.140557
3503.473924	365457.470369	45.145562
3503.691131	365441.432603	45.150567
3503.654017	365451.106912	45.155572
3503.502608	365458.560314	45.160577
3503.773355	365448.467719	45.165581
3503.709679	365453.591950	45.170586
3503.832408	365455.150152	45.175591
3503.926077	365445.848836	45.180596
3503.738452	365419.214491	45.185601
3503.807348	365425.996998	45.190605
3503.707717	365426.292765	45.195610
3503.910610	365423.741989	45.200615
3503.807885	365423.045972	45.205620
3503.583738	365432.190109	45.210625
3503.850406	365409.351259	45.215629
3503.453295	365409.897598	45.220634
3503.292826	365407.735021	45.225639
3503.280572	365410.026965	45.230644
3503.509744	365402.358008	45.235649
3503.715296	365407.134368	45.240653
3503.423621	365406.290121	45.245658
3503.960939	365406.815953	45.250663
3503.863804	365401.437557	45.255668
3503.575865	365415.120620	45.260673
3503.823604	365405.820383	45.265677
3503.483540	365410.784769	45.270682
3503.520267	365393.121728	45.275687
3503.396549	365383.854766	45.280692
3503.333334	365380.709982	45.285697
3503.750668	365374.385193	45.290701
3503.463107	365383.081392	45.295706
3503.393141	365377.546040	45.300711
3503.256090	365382.173021	45.305716
3503.347504	365383.227317	45.310721
3503.775655	365381.963959	45.315725
3503.642885	365389.567084	45.320730
3503.466148	365386.185818	45.325735
3503.555702	365383.118655	45.330740
3503.319933	365378.957990	45.335745
3503.740042	365389.246990	45.340749
3503.422043	365401.789877	45.345754
3503.704911	365396.046092	45.350759
3503.749147	365388.457255	45.355764
3503.568892	365391.666261	45.360769
3504.015458	365385.845710	45.365773
3503.804853	365376.363496	45.370778
3504.041466	365360.577062	45.375783
3503.711850	365358.542995	45.380788
3503.700906	365352.540337	45.385793
3503.898855	365349.277936	45.390797
3503.273043	365366.372895	45.395802
3503.508468	365363.740643	45.400807
3503.498901	365365.116219	45.405812
3503.559015	365363.122312	45.410817
3503.727263	365341.138603	45.415821
3503.341196	365332.523736	45.420826
3503.653443	365324.536317	45.425831
3503.553768	365336.255977	45.430836
3503.548110	365326.028951	45.435841
3503.924952	365312.917285	45.440845
3503.448634	365335.051772	45.445850
3503.616292	365336.043130	45.450855
3503.602560	365334.264439	45.455860
3503.473539	365335.557128	45.460865
3503.897414	365342.665175	45.465869
3503.811577	365333.417657	45.470874
3503.758734	365312.664705	45.475879
3503.479100	365306.195658	45.480884
3503.563989	365303.256442	45.485889
3503.829043	365301.789879	45.490893
3503.600184	365316.812109	45.495898
3503.816850	365302.224628	45.500903
3503.483382	365307.289754	45.505908
3503.413437	365307.402729	45.510913
3503.939997	365310.347343	45.515917
3503.806714	365308.002363	45.520922
3503.597122	365277.427747	45.525927
3503.566077	365279.798997	45.530932
3503.181028	365274.059014	45.535937
3503.747453	365270.229496	45.540941
3503.792282	365276.252541	45.545946
3503.800693	365276.887431	45.550951
3503.506778	365271.234812	45.555956
3503.449148	365276.663423	45.560961
3503.971813	365276.046639	45.565965
3503.769455	365291.293674	45.570970
3503.969438	365259.712907	45.575975
3503.546024	365254.055316	45.580980
3503.639293	365244.728579	45.585985
3503.949280	365242.059090	45.590989
3503.450026	365248.473468	45.595994
3503.689159	365247.163659	45.600999
3503.676978	365248.081678	45.606004
3503.621037	365252.212432	45.611009
3503.715210	365245.302637	45.616013
3503.334856	365230.555084	45.621018
3503.787276	365217.126126	45.626023
3503.671044	365219.230973	45.631028
3503.752548	365210.694823	45.636033
3504.001425	365209.765118	45.641037
3504.024393	365226.197820	45.646042
3504.038765	365214.644565	45.651047
3504.012007	365200.426292	45.656052
3504.045503	365192.075829	45.661057
3504.038098	365184.495122	45.666061
3503.845400	365187.629780	45.671066
3503.990008	365162.978203	45.676071
3504.024562	365153.024654	45.681076
3503.734342	365144.928903	45.686081
3504.254486	365132.990354	45.691085
3503.730194	365130.020216	45.696090
3503.750903	365126.531387	45.701095
3503.911473	365116.812339	45.706100
3503.587231	365109.790568	45.711105
3503.904258	365108.442999	45.716109
3503.441465	365121.441386	45.721114
3503.928864	365105.488002	45.726119
3503.776403	365113.272387	45.731124
3503.640928	365100.368866	45.736129
3503.754134	365082.286524	45.741133
3503.653774	365075.483786	45.746138
3503.544179	365070.056435	45.751143
3503.654726	365085.025085	45.756148
3503.579098	365076.081218	45.761153
3503.752507	365070.252924	45.766157
3503.482369	365082.203142	45.771162
3503.965666	365076.249529	45.776167
3503.760970	365061.601367	45.781172
3503.539787	365055.530134	45.786177
3503.808253	365045.107049	45.791181
3503.552265	365049.498435	45.796186
3503.522262	365047.137114	45.801191
3503.539058	365052.732088	45.806196
3503.667480	365048.819135	45.811201
3503.685535	365055.660622	45.816205
3503.724044	365056.748733	45.821210
3503.759474	365044.835902	45.826215
3503.655289	365040.043769	45.831220
3503.591282	365026.111204	45.836225
3503.801020	365014.450684	45.841229
3503.654417	365020.300481	45.846234
3503.839378	365019.050116	45.851239
3503.662321	365019.307240	45.856244
3503.821265	365014.575280	45.861249
3503.970438	365014.551842	45.866253
3503.755284	365002.500513	45.871258
3503.821847	364987.580456	45.876263
3503.783672	364983.719278	45.881268
3503.742115	364986.244864	45.886273
3504.027461	364993.781955	45.891277
3503.681093	364993.785971	45.896282
3503.719627	364984.111630	45.901287
3503.826166	364966.666374	45.906292
3503.787529	364952.780663	45.911297
3503.746083	364953.245337	45.916301
3503.423282	364954.136137	45.921306
3503.918535	364952.149752	45.926311
3503.667040	364960.458682	45.931316
3503.673445	364962.238836	45.936321
3503.822066	364950.435302	45.941325
3503.367561	364940.151930	45.946330
3503.527821	364932.163027	45.951335
3503.391915	364937.578610	45.956340
3503.170507	364933.110315	45.961345
3503.544653	364931.651938	45.966349
3503.401325	364935.694763	45.971354
3503.335493	364942.193324	45.976359
3503.376839	364951.600904	45.981364
3503.303875	364943.038237	45.986369
3503.380408	364945.188952	45.991373
3503.457411	364949.782137	45.996378
3503.766565	364937.647904	46.001383
3503.551752	364942.745199	46.006388
3503.400189	364944.753871	46.011393
3504.080146	364945.562477	46.016397
3503.842569	364955.497572	46.021402
3503.687614	364950.026490	46.026407
3503.489842	364961.481880	46.031412
3503.403285	364965.312182	46.036417
3503.557503	364962.692745	46.041421
3503.670602	364973.793669	46.046426
3503.658050	364953.822920	46.051431
3503.499084	364932.348719	46.056436
3503.595284	364929.305918	46.061441
3504.113331	364919.911962	46.066445
3503.647812	364931.994881	46.071450
3503.830755	364924.969231	46.076455
3503.908306	364926.839911	46.081460
3503.570517	364920.787094	46.086465
3503.595685	364902.973030	46.091469
3503.529290	364886.979901	46.096474
3503.585008	364887.861750	46.101479
3503.390571	364892.370636	46.106484
3503.576109	364892.137904	46.111489
3503.558687	364882.701376	46.116493
3503.431321	364895.366926	46.121498
3503.864710	364889.319407	46.126503
3503.763490	364897.070285	46.131508
3503.977166	364899.631856	46.136513
3504.062637	364893.919214	46.141517
3504.017948	364881.001278	46.146522
3503.989145	364856.631382	46.151527
3504.027764	364858.813538	46.156532
3503.741598	364852.777993	46.161537
3504.001920	364848.386194	46.166541
3503.536246	364833.575670	46.171546
3503.771390	364818.120041	46.176551
3503.783839	364829.669447	46.181556
3503.810258	364826.993876	46.186561
3503.660284	364824.702396	46.191565
3503.697314	364834.339672	46.196570
3503.929526	364825.219873	46.201575
3503.893674	364798.281293	46.206580
3503.713320	364792.178126	46.211585
3504.077791	364783.927925	46.216589
3503.781706	364801.123630	46.221594
3503.725084	364792.405691	46.226599
3503.989359	364787.071861	46.231604
3503.604349	364755.405120	46.236609
3503.747386	364756.476713	46.241613
3503.724117	364743.911558	46.246618
3503.838322	364744.504288	46.251623
3503.505997	364747.839152	46.256628
3503.572969	364746.810979	46.261633
3503.778061	364740.926747	46.266637
3503.421014	364757.114375	46.271642
3503.295178	364751.689552	46.276647
3503.326405	364759.394073	46.281652
3503.611595	364752.021470	46.286657
3503.749433	364759.709136	46.291661
3503.512477	364737.789193	46.296666
3503.411396	364725.770643	46.301671
3503.430937	364716.480897	46.306676
3503.628277	364721.080524	46.311681
3503.676364	364715.857192	46.316685
3503.697338	364718.907217	46.321690
3503.817558	364716.064151	46.326695
3503.501532	364721.202915	46.331700
3503.502850	364718.073326	46.336705
3503.692466	364715.448279	46.341709
3503.419409	364740.655004	46.346714
3503.819729	364719.728367	46.351719
3503.444463	364722.510270	46.356724
3503.584967	364733.098054	46.361729
3503.465012	364718.131065	46.366733
3503.743121	364698.775780	46.371738
3503.655564	364687.085844	46.376743
3503.697377	364696.417074	46.381748
3503.731181	364695.801236	46.386753
3503.939326	364689.076885	46.391757
3504.025947	364695.500494	46.396762
3503.830850	364683.344136	46.401767
3503.644653	364664.011350	46.406772
3503.702080	364666.088769	46.411777
3504.211788	364652.294382	46.416781
3503.793292	364652.437016	46.421786
3503.711766	364653.060690	46.426791
3503.799039	364662.282966	46.431796
3503.808451	364650.043382	46.436801
3503.423065	364629.673451	46.441805
3503.133790	364628.981470	46.446810
3503.507747	364618.974148	46.451815
3503.511127	364619.660730	46.456820
3503.486617	364627.272310	46.461825
3503.511703	364618.414205	46.466829
3503.624403	364620.024908	46.471834
3503.702594	364629.757493	46.476839
3503.914215	364627.230736	46.481844
3503.864867	364625.788412	46.486849
3504.151757	364621.519607	46.491853
3503.640111	364618.318445	46.496858
3503.732469	364589.552995	46.501863
3503.910478	364589.372339	46.506868
3503.427359	364590.899131	46.511873
3503.615053	364592.447092	46.516877
3503.671841	364604.956394	46.521882
3503.635508	364593.258336	46.526887
3503.694580	364592.842049	46.531892
3503.969548	364590.865029	46.536897
3503.700427	364574.776622	46.541901
3503.287423	364576.063341	46.546906
3503.779276	364567.869293	46.551911
3503.490938	364556.923480	46.556916
3503.423480	364574.719211	46.561921
3503.748576	364562.404254	46.566925
3503.660570	364578.523970	46.571930
3503.812616	364567.839304	46.576935
3503.651770	364570.663648	46.581940
3503.531606	364566.739066	46.586945
3504.026851	364559.714876	46.591949
3503.464947	364553.799213	46.596954
3503.785799	364534.666091	46.601959
3503.343496	364535.550348	46.606964
3503.162938	364524.078620	46.611969
3503.690102	364538.091070	46.616973
3503.504820	364547.025693	46.621978
3503.601710	364530.319654	46.626983
3503.439958	364537.673069	46.631988
3503.630880	364530.544323	46.636993
3503.589025	364523.426933	46.641997
3503.295312	364542.708720	46.647002
3503.720361	364535.415745	46.652007
3503.732755	364529.383846	46.657012
3503.526299	364535.701148	46.662017
3503.571179	364532.183010	46.667021
3503.508412	364547.917095	46.672026
3503.705088	364533.332527	46.677031
3503.523362	364516.059887	46.682036
3503.228817	364522.721881	46.687041
3503.450755	364506.454046	46.692045
3503.440922	364513.910665	46.697050
3503.698975	364509.799069	46.702055
3503.747834	364522.335090	46.707060
3503.975579	364510.518934	46.712065
3504.096135	364507.166934	46.717069
3503.895105	364514.094023	46.722074
3503.948748	364497.929121	46.727079
3503.803589	364476.986833	46.732084
3503.771775	364479.892558	46.737089
3503.705357	364465.196900	46.742093
3503.497419	364474.389553	46.747098
3503.662545	364472.277233	46.752103
3503.796178	364471.823714	46.757108
3503.747646	364473.561684	46.762113
3503.976106	364461.923506	46.767117
3503.712440	364450.821107	46.772122
3503.726987	364437.741020	46.777127
3503.752186	364445.115782	46.782132
3503.559606	364448.072368	46.787137
3503.837539	364442.863555	46.792141
3503.748998	364447.177640	46.797146
3503.621886	364437.376709	46.802151
3503.754365	364415.957963	46.807156
3503.401231	364398.457942	46.812161
3503.633324	364398.981152	46.817165
3503.616249	364408.576185	46.822170
3503.942006	364403.461581	46.827175
3503.684027	364412.763932	46.832180
3503.350101	364422.943365	46.837185
3503.782073	364407.685472	46.842189
3503.499691	364416.737245	46.847194
3503.634825	364425.366804	46.852199
3503.850617	364415.257224	46.857204
3503.815533	364400.403930	46.862209
3504.010016	364391.035575	46.867213
3503.673893	364394.447396	46.872218
3503.657685	364376.232572	46.877223
3503.668365	364375.951150	46.882228
3503.487836	364377.684548	46.887233
3503.635169	364376.033018	46.892237
3503.308973	364389.010020	46.897242
3503.443652	364380.032769	46.902247
3503.363164	364379.714873	46.907252
3503.295224	364384.992559	46.912257
3503.521392	364384.397193	46.917261
3503.578510	364381.894847	46.922266
3503.755047	364379.526283	46.927271
3503.590764	364368.001057	46.932276
3503.410317	364354.468346	46.937281
3503.702379	364342.362100	46.942285
3503.450127	364349.297312	46.947290
3503.641418	364347.918711	46.952295
3503.591559	364354.821927	46.957300
3503.758139	364348.612967	46.962305
3503.673061	364347.049065	46.967309
3503.517193	364350.534167	46.972314
3504.027248	364343.151393	46.977319
3503.837979	364353.078982	46.982324
3503.216875	364334.654445	46.987329
3503.336518	364318.173723	46.992333
3503.275198	364319.099529	46.997338
3503.521056	364324.632937	47.002343
3503.409795	364325.515750	47.007348
3503.464777	364320.571161	47.012353
3503.523168	364316.770991	47.017357
3503.252595	364329.383007	47.022362
3503.463235	364320.139301	47.027367
3503.417618	364318.721820	47.032372
3503.423962	364331.951590	47.037377
3503.617067	364318.359814	47.042381
3503.507864	364330.004909	47.047386
3503.482966	364326.217907	47.052391
3503.831079	364330.132207	47.057396
3503.599804	364326.734040	47.062401
3503.631515	364328.026791	47.067405
3503.736208	364337.984241	47.072410
3503.921504	364339.379930	47.077415
3504.038894	364326.945084	47.082420
3503.460519	364311.287126	47.087425
3503.876222	364297.965477	47.092429
3503.765058	364296.176705	47.097434
3503.547489	364296.618342	47.102439
3503.302969	364300.041132	47.107444
3503.352540	364300.771303	47.112449
3504.010746	364290.998852	47.117453
3503.630701	364302.915762	47.122458
3503.593406	364309.079136	47.127463
3503.844780	364298.684027	47.132468
3503.648263	364284.263313	47.137473
3503.993487	364264.795459	47.142477
3503.672978	364260.953410	47.147482
3503.863114	364260.694505	47.152487
3503.847790	364267.007072	47.157492
3503.753136	364264.808593	47.162497
3504.056590	364256.262619	47.167501
3503.368574	364252.783991	47.172506
3503.476238	364233.633559	47.177511
3503.708328	364225.327854	47.182516
3503.533723	364231.334840	47.187521
3503.797842	364230.021053	47.192525
3503.750404	364235.778943	47.197530
3504.055228	364229.573556	47.202535
3503.392166	364226.141868	47.207540
3503.711363	364226.549536	47.212545
3503.716501	364203.751425	47.217549
3503.951263	364200.228686	47.222554
3503.852836	364190.499498	47.227559
3503.605333	364190.869537	47.232564
3503.619782	364193.080990	47.237569
3503.699106	364193.526580	47.242573
3503.324322	364193.687748	47.247578
3503.718945	364197.162166	47.252583
3503.489787	364196.867772	47.257588
3503.355120	364207.346519	47.262593
3503.624528	364201.172170	47.267597
3503.281768	364196.977423	47.272602
3503.491349	364192.491809	47.277607
3503.657778	364180.201832	47.282612
3503.631480	364164.024006	47.287617
3503.406598	364155.357989	47.292621
3503.475230	364170.740664	47.297626
3504.040969	364154.698233	47.302631
3504.013561	364155.974891	47.307636
3503.585004	364165.685913	47.312641
3503.773772	364165.605328	47.317645
3503.543993	364163.097439	47.322650
3503.558203	364163.146224	47.327655
3503.525498	364139.641643	47.332660
3503.496555	364147.661103	47.337665
3503.759000	364123.015778	47.342669
3503.540268	364138.469337	47.347674
3503.714055	364127.017823	47.352679
3503.805264	364132.168604	47.357684
3503.566964	364131.214121	47.362689
3503.883490	364135.667747	47.367693
3503.610010	364140.698076	47.372698
3503.831883	364133.360827	47.377703
3503.597876	364117.699249	47.382708
3503.654220	364101.228456	47.387713
3503.538254	364097.252282	47.392717
3503.412364	364095.694823	47.397722
3503.573412	364102.284855	47.402727
3503.720338	364095.570095	47.407732
3503.498984	364099.854322	47.412737
3503.900459	364096.101670	47.417741
3503.462355	364106.399417	47.422746
3503.562431	364094.959548	47.427751
3503.463686	364107.162806	47.432756
3503.714082	364108.344661	47.437761
3503.731212	364091.981838	47.442765
3503.290480	364086.072401	47.447770
3503.457836	364065.436730	47.452775
3503.338770	364077.515991	47.457780
3503.122542	364076.558017	47.462785
3503.359957	364075.324778	47.467789
3503.024720	364103.264155	47.472794
3503.100605	364101.980122	47.477799
3503.396855	364110.024509	47.482804
3503.584738	364094.881431	47.487809
3503.438468	364104.013523	47.492813
3503.318814	364113.828383	47.497818
3503.598905	364116.074176	47.502823
3503.532519	364113.947551	47.507828
3503.428254	364118.111491	47.512833
3503.510358	364121.915200	47.517837
3503.480845	364121.334808	47.522842
3503.902002	364109.844183	47.527847
3503.239918	364104.300508	47.532852
3503.454204	364098.363853	47.537857
3503.429169	364089.106470	47.542861
3503.135106	364086.837731	47.547866
3503.607348	364100.782668	47.552871
3503.650022	364086.095084	47.557876
3503.616405	364086.685748	47.562881
3503.764448	364092.158316	47.567885
3503.410953	364098.549812	47.572890
3503.576827	364096.564574	47.577895
3503.485785	364092.050143	47.582900
3503.674459	364097.160077	47.587905
3504.039643	364095.397767	47.592909
3503.727637	364105.802797	47.597914
3503.541780	364088.479761	47.602919
3503.337090	364073.195188	47.607924
3503.269176	364082.849214	47.612929
3503.527452	364092.909655	47.617933
3503.584075	364101.882454	47.622938
3503.882344	364084.788206	47.627943
3503.813287	364065.258542	47.632948
3503.587359	364065.116298	47.637953
3503.941085	364050.430418	47.642957
3503.614501	364058.318840	47.647962
3503.668230	364057.165527	47.652967
3503.843568	364057.875819	47.657972
3503.559755	364057.742726	47.662977
3503.696677	364037.162741	47.667981
3503.519414	364035.842395	47.672986
3503.331000	364029.333301	47.677991
3503.321231	364037.324305	47.682996
3503.391282	364036.677284	47.688001
3503.626861	364020.559782	47.693005
3503.315320	364031.524517	47.698010
3503.446303	364028.145389	47.703015
3503.579264	364025.554703	47.708020
3503.620292	364025.980905	47.713025
3503.849023	364019.609413	47.718029
3503.632129	364024.707140	47.723034
3503.980624	364025.517277	47.728039
3503.770154	364034.761306	47.733044
3503.565879	364025.786683	47.738049
3503.769676	363997.257679	47.743053
3503.833970	364004.702662	47.748058
3503.476970	364003.156292	47.753063
3503.658552	363995.036636	47.758068
3503.545256	363996.479539	47.763073
3503.823318	363994.858217	47.768077
3503.835584	363997.222687	47.773082
3503.849186	363995.668616	47.778087
3503.764841	363987.947210	47.783092
3503.692140	363973.939367	47.788097
3503.851933	363959.716659	47.793101
3503.845968	363975.823617	47.798106
3503.662105	363971.883610	47.803111
3503.722308	363977.955284	47.808116
3503.597047	363967.874078	47.813121
3503.779414	363968.659592	47.818125
3503.926321	363953.141290	47.823130
3503.822595	363934.405807	47.828135
3503.802197	363939.574254	47.833140
3503.766057	363941.462948	47.838145
3503.880407	363930.478768	47.843149
3503.764195	363941.387201	47.848154
3503.518653	363917.967041	47.853159
3503.635478	363901.970046	47.858164
3503.735669	363894.143120	47.863169
3503.949454	363891.488762	47.868173
3503.646107	363899.500757	47.873178
3503.884819	363895.672046	47.878183
3503.937815	363906.986281	47.883188
3503.700743	363885.244053	47.888193
3503.649540	363860.113852	47.893197
3503.293954	363862.103938	47.898202
3503.709416	363862.394616	47.903207
3503.574337	363862.772328	47.908212
3503.410672	363860.406632	47.913217
3503.655048	363865.660449	47.918221
3503.510539	363866.446752	47.923226
3503.825196	363859.222010	47.928231
3503.974720	363864.974253	47.933236
3503.530132	363863.645275	47.938241
3503.680620	363835.760693	47.943245
3503.644299	363840.448236	47.948250
3503.704269	363827.946002	47.953255
3503.547837	363831.024131	47.958260
3503.871168	363834.000972	47.963265
3504.008186	363829.679456	47.968269
3503.710121	363843.568141	47.973274
3503.910001	363827.914203	47.978279
3503.740288	363819.570170	47.983284
3503.474776	363804.956662	47.988289
3503.669731	363797.394620	47.993293
3503.697371	363802.962589	47.998298
3503.427137	363796.135628	48.003303
3503.254414	363796.137634	48.008308
3503.552901	363797.006569	48.013313
3503.288359	363797.328417	48.018317
3503.466891	363795.722822	48.023322
3503.689972	363792.863438	48.028327
3503.505464	363794.317605	48.033332
3503.350194	363798.158868	48.038337
3503.566162	363795.351496	48.043341
3503.429357	363804.024162	48.048346
3503.675423	363807.980084	48.053351
3503.507972	363809.456998	48.058356
3503.283486	363804.607421	48.063361
3503.836791	363808.031340	48.068365
3503.497284	363812.156165	48.073370
3503.699784	363792.532568	48.078375
3503.646820	363775.748169	48.083380
3503.446897	363784.787030	48.088385
3503.737773	363766.905074	48.093389
3503.695789	363774.494115	48.098394
3503.470945	363758.830966	48.103399
3503.431748	363771.660996	48.108404
3503.605649	363763.822395	48.113409
3503.793094	363761.960952	48.118413
3503.323294	363768.548986	48.123418
3503.539937	363767.242691	48.128423
3503.849458	363764.013427	48.133428
3503.569423	363761.309909	48.138433
3503.816142	363742.824272	48.143437
3503.484005	363739.569225	48.148442
3503.784489	363731.736052	48.153447
3503.435797	363737.159972	48.158452
3503.413370	363738.461298	48.163457
3503.778973	363732.907776	48.168461
3503.307028	363735.806797	48.173466
3503.546122	363732.028899	48.178471
3503.544328	363740.553014	48.183476
3503.339103	363738.066663	48.188481
3503.773557	363737.972682	48.193485
3503.300436	363739.497921	48.198490
3503.366463	363737.375789	48.203495
3503.319311	363749.011222	48.208500
3503.485985	363737.611623	48.213505
3503.819421	363732.215849	48.218509
3503.345187	363742.366725	48.223514
3503.451123	363740.976156	48.228519
3503.342438	363743.003546	48.233524
3503.204898	363749.004736	48.238529
3503.478507	363742.142679	48.243533
3503.540234	363752.844920	48.248538
3503.795990	363751.583329	48.253543
3503.691885	363756.765029	48.258548
3503.746657	363738.258848	48.263553
3503.870093	363716.663098	48.268557
3503.560822	363720.401493	48.273562
3503.501132	363709.393887	48.278567
3503.779129	363716.703357	48.283572
3503.846144	363713.715977	48.288577
3503.993366	363710.970356	48.293581
3503.909382	363713.426388	48.298586
3503.997877	363687.358030	48.303591
3503.855715	363688.372960	48.308596
3503.687963	363680.842795	48.313601
3503.840441	363670.132408	48.318605
3503.709362	363676.437913	48.323610
3503.723002	363664.731718	48.328615
3503.789079	363641.084046	48.333620
3503.435266	363647.959088	48.338625
3503.646500	363636.552419	48.343629
3503.084989	363638.880395	48.348634
3503.451471	363637.041531	48.353639
3503.465194	363637.828267	48.358644
3503.632971	363644.315526	48.363649
3503.439068	363633.507226	48.368653
3503.473169	363642.534562	48.373658
3503.568734	363639.822547	48.378663
3503.478538	363639.073634	48.383668
3503.561845	363636.007342	48.388673
3503.560562	363642.495883	48.393677
3503.334651	363648.638276	48.398682
3503.747893	363649.768955	48.403687
3503.486884	363646.629876	48.408692
3503.454068	363659.255377	48.413697
3504.184848	363646.774265	48.418701
3503.738461	363629.873901	48.423706
3503.250895	363613.539807	48.428711
3503.410049	363603.439002	48.433716
3503.618274	363612.362486	48.438721
3503.889898	363609.139202	48.443725
3503.706290	363613.646501	48.448730
3503.476827	363604.981104	48.453735
3503.688711	363602.683245	48.458740
3503.606360	363608.344957	48.463745
3503.896508	363607.968462	48.468749
3503.508739	363610.141754	48.473754
3503.331857	363590.578047	48.478759
3503.580229	363592.930655	48.483764
3503.395537	363591.509695	48.488769
3503.564814	363582.475930	48.493773
3503.134604	363590.279040	48.498778
3503.722513	363589.219374	48.503783
3503.524162	363587.673353	48.508788
3503.095259	363587.817634	48.513793
3503.974707	363581.623095	48.518797
3503.774744	363582.519945	48.523802
3503.352819	363582.815787	48.528807
3503.461740	363583.841914	48.533812
3503.453554	363582.494825	48.538817
3503.828539	363585.438072	48.543821
3503.672452	363595.564130	48.548826
3503.821481	363588.187422	48.553831
3503.942164	363585.903979	48.558836
3503.445377	363577.229950	48.563841
3503.786878	363562.138743	48.568845
3503.779930	363556.389657	48.573850
3503.817550	363549.361326	48.578855
3503.719547	363562.964029	48.583860
3503.872652	363556.349990	48.588865
3503.822173	363551.574654	48.593869
3503.738509	363547.237111	48.598874
3503.620817	363523.796538	48.603879
3503.630886	363522.548337	48.608884
3503.243974	363523.423856	48.613889
3503.651556	363520.509843	48.618893
3503.740684	363509.885766	48.623898
3504.020237	363512.945880	48.628903
3503.612429	363527.182781	48.633908
3503.466739	363521.557399	48.638913
3503.809524	363518.399191	48.643917
3503.702680	363515.744611	48.648922
3503.559870	363491.875445	48.653927
3503.577916	363491.160306	48.658932
3503.368605	363474.044298	48.663937
3503.438790	363476.348750	48.668941
3503.740221	363487.267598	48.673946
3503.488859	363477.715100	48.678951
3503.366297	363479.948247	48.683956
3503.415024	363492.052023	48.688961
3503.741662	363486.860847	48.693965
3503.451955	363492.504467	48.698970
3503.598407	363487.138224	48.703975
3503.448065	363485.406502	48.708980
3503.181773	363495.321008	48.713985
3503.709587	363486.892087	48.718989
3503.588912	363491.313118	48.723994
3503.651928	363488.708015	48.728999
3503.411156	363498.440378	48.734004
3503.318616	363493.671685	48.739009
3503.618074	363487.390715	48.744013
3503.392036	363492.464502	48.749018
3503.461993	363484.387846	48.754023
3503.732743	363485.642832	48.759028
3503.591692	363475.513127	48.764033
3503.499350	363471.075173	48.769037
3503.615888	363471.285890	48.774042
3503.874589	363461.143874	48.779047
3503.805981	363457.338266	48.784052
3503.625976	363463.956862	48.789057
3503.790808	363466.704344	48.794061
3503.719033	363466.435952	48.799066
3503.511413	363469.471310	48.804071
3503.553845	363462.722090	48.809076
3503.379445	363443.183371	48.814081
3503.473563	363436.985744	48.819085
3503.445092	363428.517536	48.824090
3503.623693	363429.329098	48.829095
3503.160908	363429.707732	48.834100
3503.501291	363430.188391	48.839105
3503.841988	363412.527417	48.844109
3503.429106	363431.930285	48.849114
3503.491716	363424.261885	48.854119
3503.642647	363425.357706	48.859124
3503.536257	363422.016061	48.864129
3503.663978	363421.054586	48.869133
3503.509014	363436.421968	48.874138
3503.625469	363427.294747	48.879143
3503.591891	363432.872439	48.884148
3503.489114	363436.043889	48.889153
3503.939897	363428.873892	48.894157
3503.364517	363423.825307	48.899162
3503.402363	363427.178079	48.904167
3503.984452	363430.521144	48.909172
3503.168034	363407.089197	48.914177
3503.592656	363401.068312	48.919181
3503.449773	363403.177455	48.924186
3503.734837	363400.410024	48.929191
3503.927436	363403.356673	48.934196
3503.554132	363401.278535	48.939201
3503.513453	363392.379701	48.944205
3503.871178	363408.225810	48.949210
3503.535690	363399.322695	48.954215
3503.648435	363410.958379	48.959220
3503.730373	363396.086261	48.964225
3503.426169	363365.652541	48.969229
3503.634777	363371.471837	48.974234
3503.587706	363370.995987	48.979239
3503.700302	363363.930331	48.984244
3503.381920	363377.059047	48.989249
3503.557013	363367.413664	48.994253
3503.328004	363367.526345	48.999258
3503.309432	363373.712329	49.004263
3503.668444	363373.095949	49.009268
3503.282371	363375.854196	49.014273
3503.579542	363367.359940	49.019277
3503.427611	363373.083569	49.024282
3503.998758	363375.970375	49.029287
3503.788012	363371.754682	49.034292
3503.545353	363372.989059	49.039297
3503.678577	363358.643145	49.044301
3503.272090	363350.692675	49.049306
3503.427046	363340.643365	49.054311
3503.470126	363361.933372	49.059316
3503.430143	363347.563949	49.064321
3503.434090	363344.866400	49.069325
3503.365566	363344.088612	49.074330
3503.246814	363341.181464	49.079335
3503.451341	363350.029251	49.084340
3503.581447	363354.919530	49.089345
3503.528248	363344.801352	49.094349
3503.350425	363339.282804	49.099354
3503.511281	363331.649745	49.104359
3503.646585	363336.233876	49.109364
3503.547120	363333.756227	49.114369
3503.639934	363334.581353	49.119373
3503.278045	363337.920993	49.124378
3503.790702	363335.422907	49.129383
3503.629670	363332.853215	49.134388
3503.320463	363349.746209	49.139393
3503.586619	363340.926078	49.144397
3503.701831	363343.147087	49.149402
3503.262661	363347.491261	49.154407
3503.270508	363341.409036	49.159412
3503.353659	363351.828099	49.164417
3503.705739	363348.464857	49.169421
3503.229009	363352.306088	49.174426
3503.698269	363347.423122	49.179431
3503.277282	363350.085114	49.184436
3503.410517	363352.125164	49.189441
3503.576249	363354.770734	49.194445
3503.710828	363354.775048	49.199450
3503.927931	363351.509477	49.204455
3503.797553	363335.933026	49.209460
3503.381602	363322.131913	49.214465
3503.663144	363311.451927	49.219469
3503.336850	363324.581908	49.224474
3503.484276	363311.429606	49.229479
3503.667448	363317.303819	49.234484
3503.287477	363325.328027	49.239489
3503.293769	363317.185075	49.244493
3503.527579	363313.840527	49.249498
3503.581959	363318.641005	49.254503
3503.445958	363317.263227	49.259508
3503.245975	363325.131761	49.264513
3503.612024	363310.698137	49.269517
3503.708557	363326.076684	49.274522
3503.794672	363321.279731	49.279527
3503.749304	363320.116621	49.284532
3503.843478	363325.190692	49.289537
3503.509298	363302.318556	49.294541
3503.380126	363291.856160	49.299546
3503.276769	363285.180849	49.304551
3503.280894	363286.630655	49.309556
3502.787493	363299.329068	49.314561
3503.431880	363311.745829	49.319565
3503.331554	363326.977389	49.324570
3503.460655	363326.448244	49.329575
3504.016857	363329.897185	49.334580
3503.499122	363320.157768	49.339585
3503.502981	363287.308996	49.344589
3503.369826	363301.807875	49.349594
3503.488142	363287.337076	49.354599
3503.692959	363291.961110	49.359604
3503.721986	363293.534199	49.364609
3504.039090	363289.540380	49.369613
3503.528952	363301.096454	49.374618
3503.648164	363296.625039	49.379623
3503.928999	363302.789143	49.384628
3503.753043	363287.499766	49.389633
3503.967410	363272.606672	49.394637
3503.319429	363272.200374	49.399642
3503.424939	363256.942822	49.404647
3503.551001	363254.709401	49.409652
3503.429450	363267.399926	49.414657
3503.829479	363256.370422	49.419661
3503.455617	363268.388399	49.424666
3503.628039	363262.789028	49.429671
3503.776234	363258.567468	49.434676
3503.362491	363264.765050	49.439681
3503.705669	363259.749343	49.444685
3503.567148	363262.188576	49.449690
3504.064548	363256.308832	49.454695
3503.812981	363241.387610	49.459700
3503.846506	363236.777071	49.464705
3504.113212	363215.769096	49.469709
3504.175715	363224.664804	49.474714
3503.561125	363200.793739	49.479719
3503.576827	363189.748645	49.484724
3503.641861	363186.608879	49.489729
3503.628033	363181.191607	49.494733
3503.456983	363183.076216	49.499738
3503.688459	363176.958616	49.504743
3503.712399	363176.776868	49.509748
3503.777089	363181.728395	49.514753
3503.970031	363182.893913	49.519757
3503.717133	363180.084294	49.524762
3503.629417	363167.376230	49.529767
3503.818190	363150.884161	49.534772
3503.618765	363141.501492	49.539777
3503.802123	363137.630580	49.544781
3503.569724	363142.247416	49.549786
3503.402184	363138.813640	49.554791
3503.424624	363154.153070	49.559796
3503.370443	363159.403277	49.564801
3503.518001	363146.683458	49.569805
3503.809764	363149.538113	49.574810
3503.661984	363148.340301	49.579815
3503.876507	363154.031469	49.584820
3503.822688	363132.234470	49.589825
3503.791363	363115.471854	49.594829
3503.553015	363108.283531	49.599834
3503.587651	363107.667540	49.604839
3503.351952	363109.715037	49.609844
3503.424004	363114.868961	49.614849
3503.523303	363111.545664	49.619853
3503.327592	363117.988683	49.624858
3503.429523	363120.771574	49.629863
3503.438740	363120.185046	49.634868
3503.557488	363115.153914	49.639873
3503.598067	363124.460214	49.644877
3503.337617	363126.155405	49.649882
3503.263925	363116.803742	49.654887
3503.262606	363120.824276	49.659892
3503.199085	363128.238719	49.664897
3503.636586	363121.630546	49.669901
3503.500192	363122.110249	49.674906
3503.465236	363117.790410	49.679911
3503.733902	363119.045735	49.684916
3503.873744	363125.588371	49.689921
3503.681274	363127.120150	49.694925
3503.326187	363120.153837	49.699930
3503.523890	363093.915214	49.704935
3503.860609	363094.269234	49.709940
3503.327600	363096.948950	49.714945
3503.385124	363086.889544	49.719949
3503.241472	363098.998391	49.724954
3503.291486	363094.639673	49.729959
3503.417515	363092.457137	49.734964
3503.384499	363095.922913	49.739969
3503.726258	363097.472013	49.744973
3503.480937	363098.325155	49.749978
3503.594315	363094.490748	49.754983
3504.002245	363097.988591	49.759988
3503.607161	363106.829440	49.764993
3504.020359	363100.454104	49.769997
3503.611840	363089.272497	49.775002
3503.729054	363072.053831	49.780007
3503.924556	363068.079217	49.785012
3503.736708	363058.821922	49.790017
3503.895401	363056.990440	49.795021
3503.556964	363063.914026	49.800026
3503.446850	363056.120205	49.805031
3503.653917	363051.024216	49.810036
3503.576552	363071.213853	49.815041
3504.006784	363056.693671	49.820045
3503.595344	363043.629643	49.825050
3503.525360	363032.445392	49.830055
3503.498359	363029.320166	49.835060
3503.495660	363026.598205	49.840065
3503.889910	363015.493225	49.845069
3503.231282	363024.910082	49.850074
3503.572574	363026.535592	49.855079
3503.473435	363019.147138	49.860084
3503.545762	363025.776794	49.865089
3503.324323	363024.514290	49.870093
3503.633603	363028.587507	49.875098
3503.705289	363027.354996	49.880103
3503.299432	363035.485124	49.885108
3503.280236	363040.093708	49.890113
3503.571426	363025.519165	49.895117
3503.534329	363032.013454	49.900122
3503.201760	363031.938953	49.905127
3503.706701	363032.927930	49.910132
3503.502104	363034.537962	49.915137
3503.824805	363023.953180	49.920141
3503.536199	363010.895168	49.925146
3503.620115	362996.811380	49.930151
3503.616640	362999.051168	49.935156
3503.411473	362988.906048	49.940161
3503.788496	362987.498045	49.945165
3503.531100	363000.337339	49.950170
3503.312570	362997.191500	49.955175
3503.293526	362995.260893	49.960180
3503.264133	363003.331511	49.965185
3503.591469	362992.033550	49.970189
3503.242161	362994.607898	49.975194
3503.454836	363003.098244	49.980199
3503.362954	362999.856051	49.985204
3503.250206	363004.886537	49.990209
3503.579828	362998.956952	49.995213
3503.525439	363008.939839	50.000218
3503.618146	363001.724607	50.005223
3503.300985	363004.802757	50.010228
3503.472412	363013.961173	50.015233
3503.756525	363005.061807	50.020237
3503.347205	363012.759933	50.025242
3503.684075	363009.729847	50.030247
3503.621982	363008.671150	50.035252
3503.682828	363006.829690	50.040257
3504.106708	363002.564525	50.045261
3503.556843	362995.450875	50.050266
3503.795506	362994.217411	50.055271
3503.965179	362982.689930	50.060276
3503.523532	362980.062803	50.065281
3503.763018	362977.582439	50.070285
3503.526096	362987.161635	50.075290
3503.636182	362985.159725	50.080295
3503.619462	362981.600318	50.085300
3503.428077	362979.595178	50.090305
3503.880821	362960.618662	50.095309
3503.430926	362955.346634	50.100314
3503.683948	362938.666223	50.105319
3503.536068	362940.776177	50.110324
3503.507491	362948.872120	50.115329
3503.666047	362941.570136	50.120333
3503.625904	362944.477275	50.125338
3503.660027	362943.377921	50.130343
3503.651312	362950.402064	50.135348
3503.441060	362947.331246	50.140353
3503.626898	362946.640461	50.145357
3503.661900	362949.255833	50.150362
3503.555648	362945.074470	50.155367
3503.323854	362930.480798	50.160372
3503.521658	362928.694017	50.165377
3503.722309	362911.869209	50.170381
3503.205790	362917.955864	50.175386
3503.522563	362906.888551	50.180391
3503.363605	362903.071736	50.185396
3503.603777	362912.168416	50.190401
3503.370397	362904.394056	50.195405
3503.454404	362907.205238	50.200410
3503.266516	362905.581207	50.205415
3503.474560	362907.838449	50.210420
3503.523836	362904.599378	50.215425
3503.602877	362904.841471	50.220429
3503.134766	362910.767808	50.225434
3503.694468	362913.325677	50.230439
3503.681909	362907.246620	50.235444
3503.266427	362917.973608	50.240449
3503.843390	362904.473398	50.245453
3503.969360	362919.414874	50.250458
3503.813454	362908.447731	50.255463
3503.831429	362908.470479	50.260468
3503.757476	362895.098613	50.265473
3503.881022	362871.441462	50.270477
3503.435655	362873.191340	50.275482
3503.521389	362870.862499	50.280487
3503.742756	362870.598649	50.285492
3503.252183	362884.060057	50.290497
3503.726473	362866.504978	50.295501
3503.470532	362875.247541	50.300506
3503.460210	362868.303020	50.305511
3503.545947	362871.648260	50.310516
3503.346297	362879.644039	50.315521
3504.028217	362866.737889	50.320525
3503.549726	362863.785804	50.325530
3503.645829	362850.794150	50.330535
3503.607021	362847.263669	50.335540
3503.384310	362837.833730	50.340545
3503.635972	362844.664060	50.345549
3503.610045	362852.530602	50.350554
3503.437341	362846.196967	50.355559
3503.252502	362844.368897	50.360564
3503.222683	362851.192837	50.365569
3503.525790	362844.427761	50.370573
3503.289577	362855.457199	50.375578
3503.085357	362852.080089	50.380583
3503.317469	362839.321374	50.385588
3502.939545	362848.032338	50.390593
3503.594997	362853.144950	50.395597
3503.501210	362860.360666	50.400602
3503.561589	362852.285415	50.405607
3503.547226	362856.511589	50.410612
3503.484489	362854.536995	50.415617
3504.005397	362844.582390	50.420621
3503.388060	362857.682181	50.425626
3503.426066	362846.913367	50.430631
3503.533434	362851.552851	50.435636
3503.547087	362856.232594	50.440641
3503.622776	362853.981672	50.445645
3503.648250	362856.522223	50.450650
3503.723288	362854.627625	50.455655
3503.715280	362847.962622	50.460660
3503.135818	362859.198989	50.465665
3503.832235	362851.455741	50.470669
3503.335479	362837.692701	50.475674
3503.407274	362825.569991	50.480679
3503.795423	362814.873037	50.485684
3503.760627	362821.036215	50.490689
3504.132543	362812.224709	50.495693
3503.831957	362827.411759	50.500698
3503.710288	362812.520752	50.505703
3503.966475	362811.233624	50.510708
3503.551063	362796.618049	50.515713
3503.840336	362772.960093	50.520717
3503.633054	362790.625952	50.525722
3503.584887	362777.300865	50.530727
3503.442785	362767.501947	50.535732
3503.361753	362747.820953	50.540737
3503.404228	362717.662778	50.545741
3503.142235	362681.318833	50.550746
3503.172592	362627.880864	50.555751
3503.087313	362574.257558	50.560756
3502.693165	362512.286331	50.565761
3502.516217	362428.474702	50.570765
3502.148981	362368.000257	50.575770
3501.819552	362284.314254	50.580775
3502.016063	362185.430810	50.585780
3501.727158	362087.031012	50.590785
3501.527471	361973.324577	50.595789
3501.022440	361862.337849	50.600794
3500.813658	361739.701137	50.605799
3500.511192	361623.999954	50.610804
3499.514255	361499.375280	50.615809
3499.594728	361349.185700	50.620813
3498.677133	361212.868403	50.625818
3498.400661	361075.456991	50.630823
3498.192313	360932.614547	50.635828
3497.641532	360786.874137	50.640833
3497.511158	360628.725737	50.645837
3496.820715	360473.795165	50.650842
3496.493907	360312.979537	50.655847
3495.798567	360147.183365	50.660852
3495.053003	359983.048540	50.665857
3494.766358	359810.596110	50.670861
3494.119753	359644.154345	50.675866
3493.576716	359469.680097	50.680871
3493.409927	359292.906467	50.685876
3492.228754	359113.798819	50.690881
3491.942821	358932.080673	50.695885
3491.165128	358766.827150	50.700890
3490.829449	358575.954792	50.705895
3490.500643	358395.488306	50.710900
3489.425908	358214.757380	50.715905
3489.334942	358020.892339	50.720909
3488.652266	357839.131064	50.725914
3488.119131	357638.972673	50.730919
3487.638070	357440.662884	50.735924
3486.755938	357241.296026	50.740929
3486.452880	357043.287320	50.745933
3485.721143	356846.312603	50.750938
3485.260712	356642.626941	50.755943
3484.421563	356441.875914	50.760948
3483.489097	356253.837294	50.765953
3483.134513	356045.602760	50.770957
3482.554079	355845.241059	50.775962
3481.814690	355651.698340	50.780967
3480.998601	355439.386225	50.785972
3480.285390	355239.628426	50.790977
3480.069799	355032.131195	50.795981
3479.203254	354830.054776	50.800986
3478.872060	354629.928809	50.805991
3478.312954	354414.950589	50.810996
3477.181757	354212.709986	50.816001
3476.788791	353993.911863	50.821005
3476.282520	353788.466025	50.826010
3475.636158	353574.516058	50.831015
3475.061033	353359.866817	50.836020
3474.131631	353149.013757	50.841025
3473.694965	352939.049023	50.846029
3472.857631	352731.895344	50.851034
3472.250672	352516.306038	50.856039
3471.620925	352308.125332	50.861044
3470.869153	352098.766954	50.866049
3470.421808	351881.037479	50.871053
3469.528479	351665.413628	50.876058
3468.701851	351459.118569	50.881063
3467.980712	351249.421149	50.886068
3467.263043	351039.518755	50.891073
3467.062542	350828.133998	50.896077
3466.206602	350620.236964	50.901082
3465.542348	350399.430785	50.906087
3465.036108	350191.502263	50.911092
3464.069243	349972.574644	50.916097
3463.288115	349752.904152	50.921101
3462.661523	349553.900060	50.926106
3461.945395	349337.933477	50.931111
3461.122621	349129.669187	50.936116
3460.375036	348927.322387	50.941121
3460.057978	348710.297643	50.946125
3459.202752	348507.075522	50.951130
3458.517617	348303.469441	50.956135
3458.042329	348091.583074	50.961140
3457.345601	347887.264658	50.966145
3456.650305	347669.430296	50.971149
3455.986342	347464.672476	50.976154
3455.153733	347258.133476	50.981159
3454.628527	347040.549762	50.986164
3453.987909	346838.280296	50.991169
3453.655346	346620.817227	50.996173
3452.726306	346418.515514	51.001178
3451.614665	346199.010556	51.006183
3451.468287	346004.066691	51.011188
3450.223788	345787.228242	51.016193
3449.872722	345578.901689	51.021197
3448.917620	345368.837278	51.026202
3448.416984	345167.048847	51.031207
3447.648121	344961.127813	51.036212
3446.898291	344756.017546	51.041217
3446.333598	344542.834040	51.046221
3445.600822	344349.733617	51.051226
3445.034996	344140.799549	51.056231
3444.658777	343924.580492	51.061236
3443.684846	343727.978117	51.066241
3443.211089	343513.249294	51.071245
3442.753014	343305.033403	51.076250
3442.024158	343095.943260	51.081255
3441.196548	342885.773478	51.086260
3440.490115	342673.623835	51.091265
3439.937891	342461.779967	51.096269
3439.084502	342266.731898	51.101274
3438.637705	342061.004441	51.106279
3438.263029	341842.486747	51.111284
3437.261364	341638.805593	51.116289
3436.676625	341430.221458	51.121293
3435.739810	341217.212253	51.126298
3435.597551	341000.945737	51.131303
3434.762841	340800.977268	51.136308
3433.453024	340586.904854	51.141313
3433.137307	340362.950681	51.146317
3432.384408	340168.949187	51.151322
3431.743492	339955.354310	51.156327
3431.045978	339744.287733	51.161332
3430.218063	339539.121268	51.166337
3429.850271	339328.510273	51.171341
3429.260585	339136.312589	51.176346
3428.714538	338916.462587	51.181351
3427.416478	338711.164143	51.186356
3426.701472	338515.293323	51.191361
3426.636230	338307.838556	51.196365
3425.738160	338098.045579	51.201370
3425.106059	337885.027859	51.206375
3424.582531	337678.381764	51.211380
3423.768259	337480.359734	51.216385
3423.002826	337267.615639	51.221389
3422.549777	337066.429569	51.226394
3421.767045	336850.275702	51.231399
3421.283723	336632.546390	51.236404
3420.469328	336437.270546	51.241409
3420.087899	336218.378214	51.246413
3419.151082	336008.737429	51.251418
3418.106771	335801.836870	51.256423
3417.501980	335603.623362	51.261428
3416.788989	335400.385890	51.266433
3416.181028	335191.225153	51.271437
3415.343954	335000.734650	51.276442
3414.840427	334793.490919	51.281447
3414.279665	334587.859421	51.286452
3413.276624	334390.367237	51.291457
3412.690853	334187.335148	51.296461
3412.001484	333989.333979	51.301466
3411.411640	333786.810507	51.306471
3411.001475	333586.294648	51.311476
3410.310883	333378.185225	51.316481
3409.707549	333175.942147	51.321485
3408.678183	332978.679231	51.326490
3408.055638	332770.251750	51.331495
3407.852610	332561.044491	51.336500
3406.829163	332370.601702	51.341505
3406.456314	332165.900764	51.346509
3405.385533	331958.305527	51.351514
3404.692152	331763.302809	51.356519
3404.326520	331553.354561	51.361524
3403.166669	331357.813507	51.366529
3402.588407	331151.054567	51.371533
3402.019835	330963.031059	51.376538
3401.258413	330758.311199	51.381543
3400.970533	330549.722527	51.386548
3399.912070	330350.649430	51.391553
3399.442975	330152.500954	51.396557
3398.616551	329944.173943	51.401562
3397.868940	329749.454477	51.406567
3397.515391	329562.844563	51.411572
3396.707740	329351.941559	51.416577
3396.603570	329149.328272	51.421581
3395.295329	328955.586473	51.426586
3394.608452	328756.501286	51.431591
3394.370689	328551.437963	51.436596
3393.081059	328358.531860	51.441601
3392.777181	328147.749517	51.446605
3392.045990	327950.273190	51.451610
3391.105828	327746.057118	51.456615
3390.482820	327552.356164	51.461620
3389.644532	327360.216361	51.466625
3389.592086	327165.609503	51.471629
3388.583655	326975.354233	51.476634
3387.911661	326764.499051	51.481639
3387.440254	326565.526913	51.486644
3386.625601	326371.649668	51.491649
3386.250371	326163.113750	51.496653
3385.209452	325972.963050	51.501658
3384.799450	325769.218137	51.506663
3383.761499	325580.262674	51.511668
3383.292025	325381.541888	51.516673
3382.671080	325185.416083	51.521677
3381.577100	324991.248696	51.526682
3380.824595	324797.816127	51.531687
3380.349225	324604.899410	51.536692
3379.876069	324419.976577	51.541697
3379.441683	324212.870808	51.546701
3378.497747	324015.163794	51.551706
3378.075880	323821.243816	51.556711
3377.274065	323619.363252	51.561716
3376.315528	323425.527229	51.566721
3375.729807	323221.472806	51.571725
3374.881821	323044.193627	51.576730
3374.384398	322843.765283	51.581735
3373.604313	322656.901128	51.586740
3372.913118	322468.978591	51.591745
3372.437477	322277.787954	51.596749
3371.663681	322093.391338	51.601754
3371.429589	321896.101826	51.606759
3370.519260	321699.886352	51.611764
3369.369051	321514.198572	51.616769
3369.179159	321307.301701	51.621773
3368.642121	321120.930502	51.626778
3367.562840	320926.751501	51.631783
3367.406099	320725.093161	51.636788
3366.602561	320542.327558	51.641793
3365.974144	320334.351988	51.646797
3365.254344	320149.509922	51.651802
3364.600304	319950.118224	51.656807
3363.910636	319759.337929	51.661812
3363.279984	319562.335126	51.666817
3362.603620	319366.535854	51.671821
3361.785790	319173.966789	51.676826
3360.918392	318979.622797	51.681831
3360.526500	318781.994933	51.686836
3359.538165	318595.078826	51.691841
3359.114623	318403.820784	51.696845
3358.644406	318218.375201	51.701850
3357.990396	318028.451437	51.706855
3357.322887	317829.999434	51.711860
3356.425661	317643.092498	51.716865
3356.356012	317442.482657	51.721869
3355.506172	317239.245800	51.726874
3354.417000	317048.268550	51.731879
3353.917622	316852.843486	51.736884
3353.211460	316661.321108	51.741889
3352.473502	316460.636692	51.746893
3351.748069	316271.230033	51.751898
3350.974588	316079.640781	51.756903
3350.358176	315892.686080	51.761908
3349.524915	315710.399632	51.766913
3349.471724	315506.294772	51.771917
3348.413973	315325.138050	51.776922
3347.683443	315125.850261	51.781927
3347.422158	314931.427771	51.786932
3346.540753	314739.572944	51.791937
3346.156126	314542.368242	51.796941
3345.100641	314362.864586	51.801946
3344.550151	314157.995389	51.806951
3343.938841	313967.777013	51.811956
3343.130951	313777.996801	51.816961
3342.494915	313577.366973	51.821965
3341.670736	313382.037527	51.826970
3341.022346	313198.877102	51.831975
3340.421746	313005.064900	51.836980
3339.946832	312819.304537	51.841985
3339.180640	312623.098764	51.846989
3338.203602	312430.058059	51.851994
3337.845132	312242.419418	51.856999
3337.544511	312051.562830	51.862004
3336.313706	311863.730477	51.867009
3335.361223	311666.915853	51.872013
3335.356018	311477.717655	51.877018
3334.520329	311285.416521	51.882023
3333.964877	311092.561451	51.887028
3332.973309	310897.661485	51.892033
3332.778244	310711.344040	51.897037
3331.857235	310521.703406	51.902042
3331.256472	310325.696612	51.907047
3330.514240	310135.492313	51.912052
3329.521332	309946.447791	51.917057
3329.330419	309757.632624	51.922061
3328.638497	309568.718141	51.927066
3327.649674	309373.509602	51.932071
3327.100588	309191.854833	51.937076
3326.340176	309000.887636	51.942081
3325.848399	308797.934641	51.947085
3325.002359	308619.534543	51.952090
3324.553017	308429.790486	51.957095
3323.953322	308232.226711	51.962100
3323.028485	308041.564126	51.967105
3322.525802	307847.600419	51.972109
3321.747257	307669.035475	51.977114
3320.914530	307477.440715	51.982119
3320.090870	307298.576798	51.987124
3319.656837	307106.460042	51.992129
3319.166420	306909.055148	51.997133
3318.056812	306739.479547	52.002138
3317.597630	306555.871335	52.007143
3317.031436	306359.267007	52.012148
3316.031716	306176.940625	52.017153
3315.697918	305994.254008	52.022157
3314.898719	305800.435958	52.027162
3314.273747	305612.905505	52.032167
3313.675519	305433.366727	52.037172
3312.998066	305252.286842	52.042177
3312.484678	305045.638792	52.047181
3311.459909	304871.718229	52.052186
3310.973529	304685.896229	52.057191
3310.537188	304496.704594	52.062196
3309.759604	304316.810729	52.067201
3308.918423	304122.411216	52.072205
3308.178235	303938.156306	52.077210
3307.742268	303764.166691	52.082215
3306.863862	303579.576655	52.087220
3306.301605	303397.253769	52.092225
3305.963462	303206.084000	52.097229
3305.061403	303023.967186	52.102234
3304.358202	302839.144763	52.107239
3304.084116	302647.938663	52.112244
3302.861334	302453.520856	52.117249
3302.353565	302266.782319	52.122253
3301.738828	302079.602078	52.127258
3301.099106	301900.676584	52.132263
3300.425006	301708.335648	52.137268
3299.683711	301522.066054	52.142273
3299.112478	301347.101807	52.147277
3298.475807	301152.869756	52.152282
3297.904720	300967.616691	52.157287
3297.165241	300778.621027	52.162292
3296.406736	300595.154345	52.167297
3295.982534	300404.045593	52.172301
3294.996140	300219.443074	52.177306
3294.343056	300026.179967	52.182311
3293.868289	299849.339764	52.187316
3292.929447	299668.931068	52.192321
3292.756961	299458.630588	52.197325
3291.661632	299288.585641	52.202330
3290.830358	299098.278291	52.207335
3290.472653	298909.118216	52.212340
3289.550174	298730.412188	52.217345
3289.009978	298543.776307	52.222349
3288.413002	298370.111751	52.227354
3287.847116	298174.540730	52.232359
3286.969711	297993.076410	52.237364
3286.475339	297806.941832	52.242369
3285.744701	297622.932710	52.247373
3284.753310	297440.365322	52.252378
3284.123345	297262.553814	52.257383
3283.508773	297062.685388	52.262388
3282.595535	296892.736662	52.267393
3282.012223	296715.426587	52.272397
3281.338065	296546.025468	52.277402
3281.067595	296362.044169	52.282407
3280.595313	296172.084407	52.287412
3279.668644	295995.439182	52.292417
3279.073660	295808.758251	52.297421
3278.433237	295635.505473	52.302426
3277.752405	295449.168852	52.307431
3277.255915	295265.680682	52.312436
3276.158395	295087.839253	52.317441
3275.809886	294904.352814	52.322445
3274.900634	294722.788549	52.327450
3274.270356	294534.201982	52.332455
3273.722121	294339.082657	52.337460
3272.647874	294168.851459	52.342465
3272.448953	293977.267427	52.347469
3271.400927	293808.890905	52.352474
3271.157804	293623.196495	52.357479
3270.446111	293436.455486	52.362484
3269.474790	293260.833688	52.367489
3269.121349	293075.410943	52.372493
3268.297690	292906.565299	52.377498
3267.720309	292720.388199	52.382503
3267.091685	292541.324469	52.387508
3266.283124	292362.849349	52.392513
3265.656063	292175.762844	52.397517
3264.976146	292005.162020	52.402522
3264.382866	291819.801683	52.407527
3263.811521	291636.475136	52.412532
3262.791124	291456.581204	52.417537
3262.426653	291263.976936	52.422541
3261.334844	291095.325238	52.427546
3260.732068	290913.047303	52.432551
3260.633867	290728.219060	52.437556
3259.751818	290554.109221	52.442561
3259.187966	290368.284745	52.447565
3258.565878	290184.430363	52.452570
3258.069814	290001.065272	52.457575
3257.144865	289814.533505	52.462580
3256.155102	289643.725451	52.467585
3256.107467	289452.190321	52.472589
3255.189717	289279.333235	52.477594
3254.297545	289087.880524	52.482599
3253.880521	288906.947122	52.487604
3252.751593	288730.430286	52.492609
3252.079053	288541.845804	52.497613
3251.455045	288371.666772	52.502618
3250.833721	288187.352565	52.507623
3250.552626	288014.572303	52.512628
3249.922874	287835.480133	52.517633
3249.358256	287643.337997	52.522637
3248.139783	287462.148513	52.527642
3247.681420	287277.145833	52.532647
3247.192625	287100.475880	52.537652
3246.662572	286925.875265	52.542657
3245.911988	286737.225666	52.547661
3245.019718	286557.996061	52.552666
3244.311764	286379.068292	52.557671
3243.548571	286198.213604	52.562676
3242.737885	286020.065949	52.567681
3242.418818	285833.079434	52.572685
3241.988592	285668.445881	52.577690
3240.898529	285494.289721	52.582695
3240.258364	285292.021974	52.587700
3239.654218	285127.110090	52.592705
3238.974967	284951.335148	52.597709
3238.252519	284773.020156	52.602714
3237.628417	284587.991418	52.607719
3236.889595	284408.685606	52.612724
3235.849172	284238.086597	52.617729
3235.740381	284061.813551	52.622733
3234.663391	283905.711569	52.627738
3234.208202	283722.285707	52.632743
3233.780639	283541.707837	52.637748
3232.462002	283368.351021	52.642753
3232.208667	283198.925988	52.647757
3231.447686	283026.805176	52.652762
3231.094552	282841.758341	52.657767
3230.283359	282665.774185	52.662772
3229.208058	282501.521666	52.667777
3229.077232	282321.507656	52.672781
3228.068858	282153.449679	52.677786
3227.638158	281980.181147	52.682791
3227.058561	281800.212501	52.687796
3226.206145	281628.182123	52.692801
3225.739476	281447.100372	52.697805
3224.913556	281269.564559	52.702810
3224.126296	281086.343155	52.707815
3223.662722	280923.878079	52.712820
3222.594499	280750.251641	52.717825
3222.591927	280569.198103	52.722829
3221.352888	280403.850334	52.727834
3220.480418	280232.051990	52.732839
3220.522351	280056.594315	52.737844
3219.370452	279878.855049	52.742849
3219.003484	279711.688259	52.747853
3217.983805	279540.116807	52.752858
3217.764030	279364.598520	52.757863
3217.157734	279190.542111	52.762868
3216.132069	279019.251662	52.767873
3215.710868	278840.479733	52.772877
3215.069826	278666.836224	52.777882
3214.194854	278493.866407	52.782887
3213.518790	278319.795425	52.787892
3212.612333	278149.224566	52.792897
3212.277479	277964.912207	52.797901
3211.216463	277803.814520	52.802906
3210.935843	277637.423269	52.807911
3210.442814	277461.132939	52.812916
3209.324035	277292.531169	52.817921
3208.996871	277119.245299	52.822925
3208.493441	276946.140112	52.827930
3207.698758	276768.674960	52.832935
3207.034520	276587.445304	52.837940
3206.304595	276410.071754	52.842945
3205.795090	276231.084280	52.847949
3204.705164	276081.146185	52.852954
3204.258033	275893.897067	52.857959
3203.820347	275728.218175	52.862964
3203.100422	275560.903018	52.867969
3202.410210	275378.786020	52.872973
3201.547107	275213.785665	52.877978
3200.668559	275030.654257	52.882983
3200.300599	274854.394936	52.887988
3199.339247	274691.625875	52.892993
3198.820265	274508.794139	52.897997
3198.084706	274358.290592	52.903002
3197.472866	274184.616708	52.908007
3196.994747	274009.750127	52.913012
3196.116711	273835.965563	52.918017
3195.894028	273663.681827	52.923021
3194.979615	273497.823705	52.928026
3194.490191	273329.402451	52.933031
3193.905923	273149.229821	52.938036
3193.073759	272973.324179	52.943041
3192.868503	272796.045945	52.948045
3191.928425	272625.684047	52.953050
3191.526430	272451.951610	52.958055
3190.823799	272269.250956	52.963060
3189.296665	272097.835922	52.968065
3189.117968	271916.835201	52.973069
3188.110717	271746.967931	52.978074
3187.696064	271581.107328	52.983079
3186.795461	271408.268902	52.988084
3186.195881	271243.176188	52.993089
3185.885732	271069.403936	52.998093
3184.696883	270902.850942	53.003098
3184.145972	270726.340794	53.008103
3183.941300	270553.876297	53.013108
3183.082157	270388.748389	53.018113
3182.567215	270211.876091	53.023117
3181.682717	270043.645126	53.028122
3181.002882	269869.294886	53.033127
3180.421676	269702.213014	53.038132
3179.449959	269517.008600	53.043137
3179.102102	269351.316109	53.048141
3178.077357	269196.758525	53.053146
3177.630620	269016.641238	53.058151
3177.059539	268846.832855	53.063156
3175.913091	268680.986731	53.068161
3175.418625	268507.753566	53.073165
3174.912951	268333.885516	53.078170
3174.172954	268168.943010	53.083175
3173.356436	268007.934766	53.088180
3172.781736	267849.307787	53.093185
3172.197088	267677.438947	53.098189
3171.349629	267512.360823	53.103194
3170.719553	267342.001901	53.108199
3170.287083	267177.443986	53.113204
3169.514528	267017.829827	53.118209
3168.794423	266841.678565	53.123213
3168.271604	266682.508892	53.128218
3167.474879	266515.487478	53.133223
3166.973174	266344.471875	53.138228
3166.024866	266193.188414	53.143233
3165.776635	266023.864657	53.148237
3164.630510	265853.918992	53.153242
3164.077962	265689.482458	53.158247
3164.000860	265522.016453	53.163252
3162.761231	265350.303011	53.168257
3162.191790	265171.836423	53.173261
3161.778124	265018.482259	53.178266
3161.023425	264838.822660	53.183271
3160.609862	264662.037990	53.188276
3159.534277	264509.247183	53.193281
3159.177511	264329.473914	53.198285
3158.371878	264166.606120	53.203290
3157.633224	263996.647690	53.208295
3157.202599	263828.117742	53.213300
3155.850680	263672.493116	53.218305
3155.634060	263511.315171	53.223309
3155.044692	263342.963376	53.228314
3154.286351	263175.809925	53.233319
3153.823315	263015.511641	53.238324
3152.710341	262848.363530	53.243329
3152.280109	262676.752453	53.248333
3151.452682	262513.634194	53.253338
3150.555551	262351.061871	53.258343
3150.437187	262185.743209	53.263348
3149.455288	262023.897566	53.268353
3148.813437	261852.065735	53.273357
3148.167782	261684.742409	53.278362
3147.628829	261523.743779	53.283367
3147.335420	261360.032260	53.288372
3146.023615	261201.677411	53.293377
3145.708933	261018.613917	53.298381
3144.677797	260864.111408	53.303386
3144.077835	260706.866640	53.308391
3143.647523	260543.610192	53.313396
3142.675490	260376.339257	53.318401
3142.087221	260205.798763	53.323405
3141.202884	260049.745409	53.328410
3140.778378	259889.035197	53.333415
3140.224128	259732.394971	53.338420
3139.225672	259578.779376	53.343425
3138.656632	259411.216057	53.348429
3137.862424	259245.725885	53.353434
3137.358313	259096.183570	53.358439
3136.702264	258934.644681	53.363444
3136.355647	258773.591750	53.368449
3135.578839	258619.508704	53.373453
3134.902705	258451.300804	53.378458
3134.155980	258287.510071	53.383463
3133.529258	258137.554783	53.388468
3132.623964	257980.640109	53.393473
3132.163675	257808.145427	53.398477
3131.657385	257653.765510	53.403482
3131.091731	257483.019526	53.408487
3130.016628	257329.901337	53.413492
3129.378895	257172.129905	53.418497
3128.817374	257005.203730	53.423501
3128.247009	256833.440278	53.428506
3127.664211	256678.003494	53.433511
3126.851648	256515.905270	53.438516
3125.896135	256364.704329	53.443521
3125.804054	256199.257976	53.448525
3124.847127	256038.889259	53.453530
3124.008278	255880.794030	53.458535
3123.536713	255721.036360	53.463540
3122.619069	255566.595648	53.468545
3122.226289	255400.076941	53.473549
3121.413658	255245.059570	53.478554
3121.255000	255088.028789	53.483559
3120.182101	254917.237747	53.488564
3119.171654	254771.980486	53.493569
3118.923632	254608.826640	53.498573
3118.249102	254449.662351	53.503578
3117.661500	254280.195742	53.508583
3116.920118	254131.127244	53.513588
3116.462733	253969.433211	53.518593
3116.087452	253802.225447	53.523597
3114.826812	253640.455069	53.528602
3114.654133	253475.125551	53.533607
3113.943054	253310.365252	53.538612
3112.988804	253157.409291	53.543617
3112.575601	252988.552896	53.548621
3111.502124	252833.222182	53.553626
3110.866224	252670.946305	53.558631
3110.526897	252508.419903	53.563636
3109.239992	252348.794018	53.568641
3109.057673	252181.735439	53.573645
3108.230118	252024.940360	53.578650
3107.464617	251865.334260	53.583655
3107.274054	251697.564372	53.588660
3106.038043	251547.048234	53.593665
3105.493318	251385.675898	53.598669
3105.117578	251226.772699	53.603674
3104.467721	251069.975823	53.608679
3103.741823	250909.523937	53.613684
3102.957440	250757.816489	53.618689
3102.315074	250587.801728	53.623693
3101.475640	250439.643129	53.628698
3100.583607	250270.559531	53.633703
3100.022842	250110.260543	53.638708
3099.152219	249972.905082	53.643713
3098.532519	249807.573362	53.648717
3098.053786	249667.023770	53.653722
3097.418523	249507.042764	53.658727
3096.845404	249346.619155	53.663732
3096.156710	249203.454698	53.668737
3095.872682	249033.945109	53.673741
3094.865130	248880.211963	53.678746
3094.249525	248728.836232	53.683751
3093.821972	248567.371731	53.688756
3092.758248	248403.181332	53.693761
3092.299844	248252.621574	53.698765
3091.356758	248089.303735	53.703770
3090.766419	247934.894318	53.708775
3090.234502	247781.901914	53.713780
3089.329136	247629.376226	53.718785
3088.894078	247472.396103	53.723789
3088.138756	247322.087995	53.728794
3087.310144	247170.263680	53.733799
3087.027696	247016.010218	53.738804
3086.183670	246869.943960	53.743809
3085.792202	246703.535368	53.748813
3085.133466	246545.267413	53.753818
3084.303181	246385.320572	53.758823
3083.686542	246231.197235	53.763828
3082.946601	246082.161273	53.768833
3082.517994	245906.642734	53.773837
3081.975871	245757.855930	53.778842
3080.978715	245601.756247	53.783847
3080.717845	245446.278716	53.788852
3079.790029	245284.489571	53.793857
3079.047314	245120.201157	53.798861
3078.115643	244968.675638	53.803866
3077.932933	244814.892647	53.808871
3077.172452	244654.274648	53.813876
3076.533891	244499.469144	53.818881
3075.883688	244333.384460	53.823885
3075.158218	244176.963295	53.828890
3074.295785	244018.042916	53.833895
3073.842709	243860.789587	53.838900
3072.977636	243707.141336	53.843905
3072.637633	243540.804832	53.848909
3071.451963	243383.718956	53.853914
3071.220085	243226.482315	53.858919
3070.352520	243073.497306	53.863924
3069.577773	242919.479184	53.868929
3068.834166	242758.529796	53.873933
3068.131295	242608.804286	53.878938
3067.588525	242456.074198	53.883943
3067.446410	242296.150666	53.888948
3066.239581	242150.452551	53.893953
3065.624175	241993.354540	53.898957
3064.838151	241837.607911	53.903962
3064.326415	241681.894461	53.908967
3063.761100	241529.398268	53.913972
3062.668951	241379.761320	53.918977
3062.490308	241223.639227	53.923981
3061.420256	241075.119612	53.928986
3060.857557	240913.023547	53.933991
3060.436292	240768.017624	53.938996
3059.790429	240618.132736	53.944001
3059.071581	240455.603642	53.949005
3058.265251	240303.656446	53.954010
3057.481842	240144.652121	53.959015
3056.878357	239990.941631	53.964020
3056.254829	239850.628867	53.969025
3055.908866	239699.067954	53.974029
3054.769943	239543.074604	53.979034
3054.169428	239407.520594	53.984039
3053.637791	239241.169362	53.989044
3053.032237	239091.254596	53.994049
3052.378718	238936.687644	53.999053
3051.619695	238792.348791	54.004058
3050.942056	238632.845996	54.009063
3050.535375	238470.830509	54.014068
3049.546107	238329.584403	54.019073
3049.183738	238183.426522	54.024077
3048.666512	238031.742163	54.029082
3047.689535	237873.153616	54.034087
3047.167130	237714.238708	54.039092
3046.481878	237563.167263	54.044097
3045.647246	237403.309130	54.049101
3044.711331	237256.097385	54.054106
3044.216455	237113.959746	54.059111
3043.561723	236959.421219	54.064116
3042.604457	236816.924274	54.069121
3042.245759	236658.952631	54.074125
3041.787496	236510.393117	54.079130
3040.767955	236367.346428	54.084135
3040.366976	236225.042328	54.089140
3039.370099	236068.420301	54.094145
3038.850307	235913.148956	54.099149
3038.506053	235770.403613	54.104154
3037.319845	235607.726444	54.109159
3037.212366	235446.330207	54.114164
3036.122316	235310.222206	54.119169
3035.590333	235155.845148	54.124173
3034.720846	235009.313549	54.129178
3034.299870	234857.109225	54.134183
3033.686530	234713.491258	54.139188
3032.616881	234566.635493	54.144193
3032.458956	234404.994252	54.149197
3031.954621	234269.100497	54.154202
3030.987447	234105.296140	54.159207
3030.692238	233957.427473	54.164212
3029.642747	233814.643724	54.169217
3029.203170	233662.367765	54.174221
3028.263696	233503.143372	54.179226
3027.571887	233353.377730	54.184231
3027.008331	233208.557292	54.189236
3026.111293	233063.637078	54.194241
3025.651662	232921.652464	54.199245
3024.801450	232776.827117	54.204250
3024.234378	232625.413230	54.209255
3023.861592	232482.600704	54.214260
3022.990542	232338.568661	54.219265
3022.353909	232185.078535	54.224269
3021.608481	232041.179832	54.229274
3021.134268	231886.747822	54.234279
3020.349834	231736.591955	54.239284
3019.562053	231600.313934	54.244289
3018.893557	231451.133210	54.249293
3018.338017	231311.203174	54.254298
3017.899675	231153.354722	54.259303
3017.309987	230991.634753	54.264308
3016.521791	230847.846499	54.269313
3015.749124	230705.049041	54.274317
3015.157658	230554.839070	54.279322
3014.365675	230411.153948	54.284327
3013.716722	230260.062383	54.289332
3012.812957	230113.543661	54.294337
3012.431705	229959.736696	54.299341
3011.320493	229818.318242	54.304346
3010.873765	229686.419461	54.309351
3010.165747	229534.345438	54.314356
3009.451320	229395.130955	54.319361
3008.987961	229242.560384	54.324365
3008.329679	229099.365422	54.329370
3007.851116	228959.783278	54.334375
3007.390758	228806.449126	54.339380
3006.110965	228659.075684	54.344385
3005.658514	228509.483668	54.349389
3005.335860	228371.889246	54.354394
3004.568536	228221.736485	54.359399
3004.042027	228061.183018	54.364404
3003.056594	227914.706312	54.369409
3002.532216	227766.018109	54.374413
3001.677198	227633.754184	54.379418
3001.252116	227485.458128	54.384423
3000.143426	227332.203740	54.389428
2999.622372	227192.325619	54.394433
2999.090373	227042.010354	54.399437
2998.439245	226905.030413	54.404442
2997.589420	226762.429773	54.409447
2997.183543	226607.054006	54.414452
2996.272139	226466.016742	54.419457
2995.782732	226328.490185	54.424461
2995.229084	226182.724667	54.429466
2994.390910	226027.532979	54.434471
2993.915904	225885.167296	54.439476
2993.173079	225747.656352	54.444481
2992.657891	225587.627719	54.449485
2991.793426	225439.621237	54.454490
2991.202522	225301.946951	54.459495
2990.491001	225154.107727	54.464500
2989.424890	225013.784862	54.469505
2989.260241	224860.576521	54.474509
2988.305151	224728.638559	54.479514
2987.472072	224573.970750	54.484519
2987.301869	224431.699371	54.489524
2986.560912	224297.704110	54.494529
2986.110827	224145.280658	54.499533
2985.584575	223999.552880	54.504538
2984.710618	223845.898624	54.509543
2984.194417	223694.377606	54.514548
2983.824575	223542.922818	54.519553
2983.002436	223391.208939	54.524557
2982.258369	223245.631594	54.529562
2981.017819	223097.638034	54.534567
2980.744227	222947.403961	54.539572
2979.901064	222809.353799	54.544577
2979.311061	222653.441900	54.549581
2978.532966	222506.674702	54.554586
2977.795374	222360.754271	54.559591
2977.102493	222207.418259	54.564596
2976.356097	222071.709113	54.569601
2976.073563	221928.759888	54.574605
2975.406655	221781.327245	54.579610
2974.679544	221637.150506	54.584615
2973.978867	221488.743580	54.589620
2972.874734	221350.329992	54.594625
2972.863708	221198.148296	54.599629
2971.818273	221043.699297	54.604634
2971.150711	220913.631701	54.609639
2970.498855	220773.594551	54.614644
2969.421568	220628.482256	54.619649
2969.190321	220484.509261	54.624653
2968.273586	220349.988550	54.629658
2967.865114	220206.884297	54.634663
2967.389619	220061.665103	54.639668
2966.430726	219922.556491	54.644673
2965.651162	219769.977453	54.649677
2965.008337	219632.639660	54.654682
2964.498517	219492.951586	54.659687
2963.474253	219359.939037	54.664692
2962.668524	219221.902227	54.669697
2962.485410	219080.419296	54.674701
2961.534696	218944.684512	54.679706
2961.128065	218811.396973	54.684711
2960.798805	218670.829024	54.689716
2959.228166	218538.910086	54.694721
2959.394131	218393.758126	54.699725
2958.756013	218248.084567	54.704730
2957.725354	218102.218866	54.709735
2957.113512	217972.033091	54.714740
2956.496384	217832.899828	54.719745
2956.234793	217687.205987	54.724749
2955.383451	217548.619521	54.729754
2954.447205	217406.126227	54.734759
2954.131963	217255.031928	54.739764
2953.223727	217117.231784	54.744769
2952.742605	216979.377018	54.749773
2951.823815	216835.596489	54.754778
2951.074114	216695.086270	54.759783
2950.492099	216548.032600	54.764788
2949.464457	216412.149349	54.769793
2949.169738	216268.933084	54.774797
2948.393329	216146.299472	54.779802
2947.521176	216004.779000	54.784807
2947.327162	215861.013025	54.789812
2946.515161	215728.877414	54.794817
2945.563221	215592.678298	54.799821
2945.058073	215460.494622	54.804826
2944.391151	215322.150688	54.809831
2943.561569	215183.387286	54.814836
2942.921720	215036.702396	54.819841
2942.383202	214904.843294	54.824845
2941.564938	214774.708905	54.829850
2940.928127	214638.512720	54.834855
2940.538407	214499.821088	54.839860
2939.823269	214372.382318	54.844865
2939.405473	214238.545218	54.849869
2938.682560	214094.001176	54.854874
2937.699439	213954.259062	54.859879
2936.971604	213806.508867	54.864884
2936.353103	213680.927183	54.869889
2935.818120	213540.618580	54.874893
2935.242214	213410.181176	54.879898
2934.745139	213275.887613	54.884903
2934.197667	213130.643290	54.889908
2933.224053	212989.743435	54.894913
2932.649256	212851.364559	54.899917
2932.151325	212714.615736	54.904922
2931.171958	212572.406688	54.909927
2930.564081	212430.775538	54.914932
2929.675806	212296.291355	54.919937
2929.480102	212160.170431	54.924941
2928.436169	212019.092883	54.929946
2927.698448	211889.549634	54.934951
2927.169401	211752.871400	54.939956
2926.480117	211619.044428	54.944961
2925.659010	211473.910764	54.949965
2925.013473	211349.814279	54.954970
2924.604710	211211.170786	54.959975
2924.120329	211075.301505	54.964980
2923.278253	210951.287823	54.969985
2922.885468	210808.544320	54.974989
2921.901783	210664.825564	54.979994
2921.070513	210526.975938	54.984999
2920.687737	210391.690235	54.990004
2919.756788	210262.308159	54.995009
2919.382365	210119.397843	55.000013
2918.634704	209991.183703	55.005018
2918.065914	209845.071972	55.010023
2917.369195	209708.144678	55.015028
2916.238989	209572.329977	55.020033
2915.767215	209433.114897	55.025037
2915.269117	209316.202833	55.030042
2914.448507	209181.739988	55.035047
2913.990664	209040.270826	55.040052
2913.175087	208918.293357	55.045057
2912.573955	208777.891129	55.050061
2911.872876	208644.479628	55.055066
2911.253815	208516.808174	55.060071
2910.888112	208376.433224	55.065076
2909.962456	208247.309057	55.070081
2909.532662	208097.284908	55.075085
2908.870738	207964.237780	55.080090
2908.127419	207824.522067	55.085095
2907.575933	207690.579876	55.090100
2906.563825	207557.461815	55.095105
2905.816124	207414.985957	55.100109
2905.398980	207287.896012	55.105114
2904.491729	207149.162346	55.110119
2904.317820	207007.105682	55.115124
2903.171400	206881.595673	55.120129
2902.958782	206750.465486	55.125133
2901.941987	206609.434112	55.130138
2901.232409	206472.668840	55.135143
2900.514419	206336.096118	55.140148
2900.292947	206204.574001	55.145153
2899.648837	206062.199506	55.150157
2898.683696	205934.002895	55.155162
2898.101642	205800.604302	55.160167
2897.597821	205654.174202	55.165172
2896.463538	205522.301798	55.170177
2895.775933	205376.156026	55.175181
2895.460816	205254.666727	55.180186
2894.810658	205121.496814	55.185191
2894.124849	204995.879701	55.190196
2893.027336	204855.438005	55.195201
2892.458564	204720.168972	55.200205
2891.903584	204601.684291	55.205210
2891.013558	204457.100054	55.210215
2890.328226	204322.003125	55.215220
2889.820416	204208.042386	55.220225
2889.314106	204079.255421	55.225229
2888.902015	203949.626614	55.230234
2888.191159	203809.266229	55.235239
2887.413562	203678.359650	55.240244
2886.586056	203545.845041	55.245249
2886.440832	203404.963392	55.250253
2885.380146	203281.038336	55.255258
2884.529648	203141.312563	55.260263
2884.080765	203006.550359	55.265268
2883.159637	202882.807694	55.270273
2882.546135	202740.665603	55.275277
2881.913478	202618.761296	55.280282
2881.131763	202485.363820	55.285287
2880.834580	202361.256254	55.290292
2879.625336	202232.686592	55.295297
2879.418485	202094.783113	55.300301
2878.566997	201964.783018	55.305306
2877.816275	201842.224623	55.310311
2877.558891	201704.291931	55.315316
2876.609601	201579.971215	55.320321
2875.874269	201442.903855	55.325325
2875.353624	201314.583596	55.330330
2874.694165	201177.466701	55.335335
2874.141664	201054.725950	55.340340
2873.284382	200922.260435	55.345345
2872.840966	200789.958766	55.350349
2872.063932	200669.023291	55.355354
2871.340956	200539.018924	55.360359
2870.816426	200407.825418	55.365364
2869.910915	200273.129417	55.370369
2869.368965	200144.484403	55.375373
2868.554996	200016.760822	55.380378
2868.046904	199885.795028	55.385383
2867.757897	199759.401443	55.390388
2866.787626	199628.687613	55.395393
2866.249662	199486.491034	55.400397
2865.622478	199359.566571	55.405402
2864.660184	199231.232068	55.410407
2864.217818	199090.484801	55.415412
2863.554390	198965.755744	55.420417
2862.733605	198835.236498	55.425421
2862.161478	198708.419381	55.430426
2861.463493	198577.054186	55.435431
2860.845696	198439.085033	55.440436
2859.842650	198323.586029	55.445441
2859.294083	198199.387751	55.450445
2858.621307	198064.380478	55.455450
2857.964567	197934.588237	55.460455
2857.637034	197814.504191	55.465460
2856.946334	197680.302406	55.470465
2856.203696	197547.585271	55.475469
2855.273988	197415.190766	55.480474
2854.708659	197284.405839	55.485479
2854.598164	197153.142020	55.490484
2853.256160	197028.995799	55.495489
2853.361015	196895.369898	55.500493
2852.317967	196765.870764	55.505498
2851.485062	196633.742851	55.510503
2851.118203	196495.433664	55.515508
2850.374469	196372.593973	55.520513
2849.760655	196235.584319	55.525517
2848.902448	196102.901886	55.530522
2848.038697	195975.488600	55.535527
2847.419635	195838.289964	55.540532
2846.870936	195728.819749	55.545537
2846.231487	195582.972427	55.550541
2845.693087	195464.810399	55.555546
2844.729590	195330.377950	55.560551
2844.458393	195197.184993	55.565556
2843.507996	195070.538409	55.570561
2842.794377	194931.015917	55.575565
2841.882192	194814.912288	55.580570
2841.421531	194688.214548	55.585575
2840.868091	194565.883466	55.590580
2840.041595	194435.465231	55.595585
2839.364993	194302.656921	55.600589
2838.545119	194179.796383	55.605594
2837.967692	194060.562260	55.610599
2837.482604	193934.493753	55.615604
2836.696229	193808.600516	55.620609
2835.854808	193679.497166	55.625613
2835.247331	193561.248727	55.630618
2834.995521	193430.105895	55.635623
2834.529290	193298.081251	55.640628
2833.492128	193187.523298	55.645633
2832.812268	193049.667488	55.650637
2832.642079	192922.279290	55.655642
2831.527230	192798.272834	55.660647
2830.978031	192667.077319	55.665652
2830.103371	192538.185773	55.670657
2829.599725	192405.138817	55.675661
2828.855396	192289.052638	55.680666
2828.120300	192166.514453	55.685671
2827.996271	192028.827931	55.690676
2826.648073	191913.245425	55.695681
2826.392701	191777.488925	55.700685
2825.859810	191652.375320	55.705690
2825.013060	191523.303889	55.710695
2824.386936	191395.737379	55.715700
2823.772736	191272.075359	55.720705
2823.185529	191131.996401	55.725709
2822.503629	191019.287730	55.730714
2821.813044	190874.556470	55.735719
2821.483127	190737.542356	55.740724
2820.344374	190613.507057	55.745729
2819.446469	190476.647252	55.750733
2819.109403	190358.007455	55.755738
2818.425897	190236.471082	55.760743
2818.182646	190113.134967	55.765748
2817.168733	189983.877827	55.770753
2816.861168	189840.005065	55.775757
2816.095784	189703.851681	55.780762
2814.914590	189578.299037	55.785767
2814.427138	189439.646884	55.790772
2813.690578	189322.599657	55.795777
2813.351178	189190.578785	55.800781
2812.756368	189061.474057	55.805786
2812.082308	188926.936937	55.810791
2811.120606	188796.466101	55.815796
2810.587772	188673.255912	55.820801
2810.070230	188535.667142	55.825805
2809.267261	188407.576804	55.830810
2808.104824	188284.454624	55.835815
2807.813009	188146.882130	55.840820
2807.121046	188016.294403	55.845825
2806.766302	187898.770399	55.850829
2805.923639	187774.377566	55.855834
2805.141247	187634.606976	55.860839
2804.738463	187502.651765	55.865844
2804.067718	187373.830870	55.870849
2803.635634	187236.703105	55.875853
2802.602561	187109.047160	55.880858
2801.760641	186981.692068	55.885863
2801.445047	186850.055677	55.890868
2800.426002	186723.136457	55.895873
2799.888405	186592.159343	55.900877
2799.350609	186459.605108	55.905882
2798.459102	186332.743096	55.910887
2797.788754	186200.236046	55.915892
2796.920516	186082.060107	55.920897
2796.492987	185954.387788	55.925901
2795.901105	185836.664865	55.930906
2795.138718	185711.234411	55.935911
2794.644155	185575.330060	55.940916
2793.816521	185445.865160	55.945921
2793.051819	185313.922658	55.950925
2792.487740	185191.121057	55.955930
2791.946324	185065.988148	55.960935
2791.334262	184942.482411	55.965940
2790.310616	184815.760047	55.970945
2790.055883	184679.807672	55.975949
2789.316811	184556.755637	55.980954
2788.824370	184428.970675	55.985959
2788.237971	184302.371323	55.990964
2787.175534	184176.738220	55.995969
2786.749817	184043.867969	56.000973
2785.996236	183918.988113	56.005978
2785.138309	183784.062639	56.010983
2784.976857	183654.242948	56.015988
2784.086098	183540.211616	56.020993
2783.497840	183408.310366	56.025997
2782.585194	183279.145036	56.031002
2782.033316	183154.248097	56.036007
2781.665399	183018.534954	56.041012
2780.779970	182892.699344	56.046017
2780.144764	182765.450599	56.051021
2779.072719	182636.286951	56.056026
2778.668062	182504.181221	56.061031
2778.416489	182381.681307	56.066036
2777.210200	182255.173252	56.071041
2777.232274	182124.616613	56.076045
2776.261639	181989.905274	56.081050
2775.497077	181857.922098	56.086055
2774.774702	181739.823576	56.091060
2774.356601	181601.133404	56.096065
2773.549605	181470.099445	56.101069
2772.753975	181345.691475	56.106074
2772.122985	181212.747776	56.111079
2771.662681	181082.181614	56.116084
2770.761897	180957.765971	56.121089
2770.342193	180820.274263	56.126093
2769.403059	180686.223433	56.131098
2768.414625	180564.773922	56.136103
2768.234340	180420.249402	56.141108
2767.581351	180299.345359	56.146113
2766.916113	180166.893671	56.151117
2766.241260	180043.996741	56.156122
2765.429851	179918.476011	56.161127
2765.248124	179779.283600	56.166132
2764.099380	179652.354276	56.171137
2763.072282	179523.052863	56.176141
2762.816920	179395.690236	56.181146
2762.034554	179274.504303	56.186151
2761.455602	179140.592058	56.191156
2760.594280	179020.487826	56.196161
2760.105495	178891.115789	56.201165
2759.094840	178767.690620	56.206170
2758.723728	178646.975569	56.211175
2758.236212	178506.283952	56.216180
2757.580406	178394.124188	56.221185
2757.108403	178263.810158	56.226189
2756.500909	178133.034650	56.231194
2755.864635	178003.841329	56.236199
2755.476584	177871.798080	56.241204
2754.374981	177745.719220	56.246209
2753.719958	177598.532094	56.251213
2752.941654	177481.319130	56.256218
2752.350806	177351.700887	56.261223
2751.957368	177215.921077	56.266228
2751.288512	177091.594507	56.271233
2750.681792	176957.184847	56.276237
2749.884384	176820.020328	56.281242
2748.964526	176686.487893	56.286247
2748.740102	176556.839525	56.291252
2747.837331	176425.658257	56.296257
2747.488279	176286.631100	56.301261
2746.684363	176159.988423	56.306266
2745.925711	176022.477000	56.311271
2744.999946	175886.022739	56.316276
2744.418247	175757.031266	56.321281
2743.703637	175624.945146	56.326285
2743.002840	175501.416992	56.331290
2741.890068	175374.240602	56.336295
2741.619764	175245.137822	56.341300
2741.188504	175120.308975	56.346305
2740.639853	174983.925173	56.351309
2739.583149	174857.759001	56.356314
2738.899606	174736.977640	56.361319
2738.566000	174607.836034	56.366324
2737.947737	174474.708183	56.371329
2737.262179	174336.923775	56.376333
2736.870828	174205.592314	56.381338
2735.888364	174067.970321	56.386343
2735.511043	173936.713822	56.391348
2734.271645	173803.305028	56.396353
2733.825266	173679.475038	56.401357
2733.261861	173546.684951	56.406362
2732.447012	173416.682246	56.411367
2731.958269	173278.654076	56.416372
2731.419548	173149.244402	56.421377
2730.644077	173022.314503	56.426381
2729.864467	172886.610282	56.431386
2729.294687	172760.373556	56.436391
2728.819565	172629.950777	56.441396
2727.820467	172493.799386	56.446401
2727.127299	172361.364461	56.451405
2726.591465	172234.513575	56.456410
2725.689991	172109.145399	56.461415
2725.378228	171978.330072	56.466420
2724.755792	171847.869614	56.471425
2724.187710	171714.081691	56.476429
2723.495908	171576.473130	56.481434
2722.484337	171435.456551	56.486439
2722.115808	171307.882680	56.491444
2721.346834	171189.389292	56.496449
2720.896089	171050.930472	56.501453
2720.327106	170911.638812	56.506458
2719.331153	170778.354248	56.511463
2718.958490	170645.772586	56.516468
2718.176950	170513.739399	56.521473
2717.732302	170377.978040	56.526477
2717.128043	170243.870226	56.531482
2716.570015	170096.161032	56.536487
2716.135095	169961.976497	56.541492
2715.059907	169823.379337	56.546497
2714.615790	169678.680323	56.551501
2713.761043	169545.988032	56.556506
2712.974399	169404.180168	56.561511
2712.701582	169268.344610	56.566516
2711.691803	169135.411240	56.571521
2711.159840	168989.011972	56.576525
2710.314437	168855.366832	56.581530
2709.660527	168715.028329	56.586535
2708.905684	168580.263459	56.591540
2707.873804	168451.392541	56.596545
2707.599154	168318.981373	56.601549
2706.964415	168182.227831	56.606554
2706.078499	168051.694724	56.611559
2705.893639	167911.793523	56.616564
2704.925405	167778.705697	56.621569
2704.727136	167639.685045	56.626573
2703.888711	167509.960115	56.631578
2703.284790	167367.927407	56.636583
2702.751436	167233.729880	56.641588
2701.840747	167096.261003	56.646593
2701.167461	166947.730249	56.651597
2700.803193	166815.694574	56.656602
2700.047982	166675.303367	56.661607
2699.254676	166541.848862	56.666612
2698.237019	166397.825388	56.671617
2697.882763	166254.396737	56.676621
2697.078411	166120.144391	56.681626
2696.314009	165984.309456	56.686631
2695.521440	165841.625758	56.691636
2694.588892	165724.192485	56.696641
2694.179684	165581.906809	56.701645
2693.735222	165451.656112	56.706650
2693.098704	165313.323845	56.711655
2692.586203	165174.565555	56.716660
2692.117883	165043.480853	56.721665
2691.620629	164898.554238	56.726669
2690.762758	164761.441624	56.731674
2689.813262	164622.093444	56.736679
2689.282396	164487.358647	56.741684
2688.644673	164350.263547	56.746689
2688.003495	164203.989231	56.751693
2687.685568	164072.655284	56.756698
2686.518722	163936.014293	56.761703
2686.027489	163783.258698	56.766708
2685.424033	163646.936407	56.771713
2684.768708	163502.688797	56.776717
2683.677730	163368.377435	56.781722
2683.233337	163229.310544	56.786727
2682.912938	163093.593928	56.791732
2681.757447	162961.760935	56.796737
2681.422676	162813.345733	56.801741
2680.542353	162680.898010	56.806746
2680.036478	162537.202707	56.811751
2679.411643	162396.959717	56.816756
2678.679827	162262.709979	56.821761
2678.256069	162124.381491	56.826765
2677.459356	161985.654907	56.831770
2676.743279	161843.877380	56.836775
2676.529335	161701.118153	56.841780
2675.383939	161568.500372	56.846785
2675.016338	161416.574301	56.851789
2674.390435	161267.334315	56.856794
2673.756348	161133.632730	56.861799
2672.847136	160990.503355	56.866804
2672.456804	160841.685526	56.871809
2671.679669	160688.403480	56.876813
2670.802795	160550.839402	56.881818
2670.220931	160418.912154	56.886823
2669.946885	160268.819638	56.891828
2668.884477	160130.917887	56.896833
2668.364019	159979.937540	56.901837
2667.750384	159846.644390	56.906842
2666.834520	159699.872494	56.911847
2666.318476	159558.517345	56.916852
2665.361086	159418.262471	56.921857
2665.146702	159274.330710	56.926861
2664.327977	159136.495947	56.931866
2663.603807	158996.447358	56.936871
2663.157242	158845.752569	56.941876
2662.249106	158711.773017	56.946881
2661.834578	158553.916928	56.951885
2661.203783	158416.589172	56.956890
2660.449478	158272.708929	56.961895
2659.809442	158126.827964	56.966900
2658.902989	157981.561899	56.971905
2658.513835	157835.426288	56.976909
2657.662474	157703.234124	56.981914
2656.763250	157560.829042	56.986919
2656.486812	157410.660152	56.991924
2655.749012	157267.518793	56.996929
2655.105493	157116.926261	57.001933
2654.389152	156993.309088	57.006938
2653.736741	156838.651185	57.011943
2653.355016	156698.214370	57.016948
2652.145635	156566.350246	57.021953
2651.833526	156416.343885	57.026957
2651.344504	156271.133291	57.031962
2650.120588	156129.357625	57.036967
2649.959868	155984.401322	57.041972
2649.133020	155847.127562	57.046977
2648.246735	155699.007719	57.051981
2648.016447	155556.670214	57.056986
2647.466469	155402.307657	57.061991
2646.395661	155266.155404	57.066996
2645.669727	155133.965980	57.072001
2644.848713	154979.749981	57.077005
2644.357169	154844.677119	57.082010
2643.754608	154702.948780	57.087015
2643.288727	154551.564004	57.092020
2642.431609	154411.339052	57.097025
2641.908649	154278.129314	57.102029
2641.084949	154138.052742	57.107034
2640.286849	153993.040689	57.112039
2640.385791	153838.251958	57.117044
2639.431682	153692.719334	57.122049
2638.966155	153539.572190	57.127053
2638.217676	153396.486955	57.132058
2637.265407	153255.087062	57.137063
2636.924990	153112.319720	57.142068
2636.224354	152968.211856	57.147073
2635.491426	152812.873282	57.152077
2634.698116	152666.302781	57.157082
2633.799897	152521.389243	57.162087
2633.257705	152371.005148	57.167092
2632.507154	152239.263202	57.172097
2632.159693	152080.244431	57.177101
2631.461326	151933.369782	57.182106
2630.739300	151788.507798	57.187111
2630.436038	151637.733282	57.192116
2629.652845	151498.449447	57.197121
2629.069458	151334.057019	57.202125
2628.300694	151191.098909	57.207130
2627.480108	151037.676400	57.212135
2626.817287	150887.750330	57.217140
2626.100047	150748.840530	57.222145
2625.466097	150601.554901	57.227149
2624.668950	150450.876803	57.232154
2624.284139	150302.116816	57.237159
2623.901631	150150.497417	57.242164
2623.001284	150013.322887	57.247169
2622.311721	149860.088508	57.252173
2621.246268	149720.551938	57.257178
2621.126011	149560.746806	57.262183
2620.223768	149405.171569	57.267188
2619.265078	149266.827449	57.272193
2618.800325	149121.415437	57.277197
2618.403218	148968.761698	57.282202
2617.772641	148835.857905	57.287207
2617.058858	148613.468939	57.292212
2616.355622	148467.220726	57.297217
2615.657579	148308.097971	57.302221
2615.046960	148164.403713	57.307226
2614.441066	148013.554156	57.312231
2613.708066	147865.432466	57.317236
2612.682316	147734.159060	57.322241
2612.374741	147568.699893	57.327245
2611.552519	147425.449171	57.332250
2610.879906	147273.584268	57.337255
2610.521832	147121.987965	57.342260
2609.513417	146977.650398	57.347265
2609.192863	146829.366500	57.352269
2608.555750	146676.367763	57.357274
2607.865020	146528.169349	57.362279
2607.686890	146378.390811	57.367284
2606.990627	146219.786545	57.372289
2606.083613	146064.088540	57.377293
2605.497701	145907.476265	57.382298
2604.451004	145756.669157	57.387303
2604.006967	145598.765122	57.392308
2602.930571	145439.094007	57.397313
2602.620037	145293.204847	57.402317
2601.727075	145148.221963	57.407322
2601.208762	145005.760076	57.412327
2600.520352	144841.582783	57.417332
2599.872777	144686.968788	57.422337
2599.411390	144534.079710	57.427341
2598.680568	144383.432491	57.432346
2598.085436	144236.462389	57.437351
2597.169560	144077.382766	57.442356
2597.068408	143925.659510	57.447361
2596.326496	143765.524619	57.452365
2595.306443	143608.306475	57.457370
2594.423930	143448.830868	57.462375
2593.901297	143295.423896	57.467380
2592.951774	143160.434361	57.472385
2592.833178	142997.561603	57.477389
2592.231811	142848.184752	57.482394
2591.617830	142699.128298	57.487399
2590.955112	142543.104239	57.492404
2590.180462	142384.392171	57.497409
2589.767069	142224.632555	57.502413
2588.815568	142073.269184	57.507418
2588.340843	141907.459879	57.512423
2587.729490	141740.046693	57.517428
2586.884569	141599.507426	57.522433
2586.252966	141445.872848	57.527437
2585.816547	141275.918629	57.532442
2585.093119	141121.093144	57.537447
2584.727980	140961.548506	57.542452
2583.725664	140795.778041	57.547457
2583.075175	140646.356223	57.552461
2582.481715	140483.826246	57.557466
2581.425914	140322.069236	57.562471
2580.824305	140172.527663	57.567476
2580.249169	140018.586438	57.572481
2579.652564	139865.856445	57.577485
2578.719274	139708.327027	57.582490
2578.156297	139551.641847	57.587495
2577.610522	139393.328454	57.592500
2576.805893	139240.088275	57.597505
2576.434305	139072.194481	57.602509
2575.604062	138922.695368	57.607514
2574.795210	138769.610735	57.612519
2574.644003	138619.865772	57.617524
2573.785887	138450.604186	57.622529
2573.151401	138293.936935	57.627533
2572.413389	138139.408646	57.632538
2571.479612	137982.078992	57.637543
2571.191055	137820.582371	57.642548
2570.107883	137673.518135	57.647553
2569.531873	137506.580318	57.652557
2569.067763	137349.878353	57.657562
2568.025569	137195.250746	57.662567
2567.552858	137040.940244	57.667572
2567.165808	136898.406698	57.672577
2566.620563	136740.628249	57.677581
2565.851630	136571.630081	57.682586
2564.993171	136409.253275	57.687591
2564.380394	136254.219553	57.692596
2563.613184	136094.536019	57.697601
2563.317311	135934.765956	57.702605
2562.578791	135780.478802	57.707610
2561.564895	135633.172433	57.712615
2560.893009	135468.764071	57.717620
2560.180034	135312.125142	57.722625
2559.777961	135152.935160	57.727629
2559.016049	135002.809943	57.732634
2558.236984	134845.485306	57.737639
2557.654082	134682.197910	57.742644
2556.905432	134537.052770	57.747649
2556.905245	134372.747420	57.752653
2556.013472	134215.228117	57.757658
2555.202345	134061.418933	57.762663
2554.693703	133892.115618	57.767668
2553.679331	133738.746870	57.772673
2553.352916	133577.698925	57.777677
2552.648444	133422.656767	57.782682
2552.002499	133262.868006	57.787687
2551.453774	133102.963106	57.792692
2550.604874	132958.210203	57.797697
2549.907441	132781.880649	57.802701
2549.540738	132623.651736	57.807706
2548.797384	132462.422092	57.812711
2547.999836	132294.380747	57.817716
2547.360411	132141.037361	57.822721
2546.683542	131973.664713	57.827725
2545.991900	131813.649970	57.832730
2545.064558	131660.049961	57.837735
2544.841458	131494.068973	57.842740
2543.655833	131343.534707	57.847745
2543.379578	131181.692126	57.852749
2542.727137	131018.678013	57.857754
2542.130950	130865.626825	57.862759
2541.425418	130698.520302	57.867764
2540.485330	130539.238048	57.872769
2539.968900	130379.965762	57.877773
2539.127746	130227.363323	57.882778
2538.857953	130069.527083	57.887783
2538.114367	129898.112872	57.892788
2537.406752	129742.341978	57.897793
2536.892401	129589.335586	57.902797
2536.189207	129423.747737	57.907802
2535.386238	129255.915897	57.912807
2534.785960	129109.123874	57.917812
2534.238100	128940.529547	57.922817
2533.788230	128765.621098	57.927821
2532.682124	128620.016801	57.932826
2532.242718	128453.059343	57.937831
2531.884068	128290.243193	57.942836
2530.788220	128120.356336	57.947841
2530.039225	127957.845320	57.952845
2529.429198	127803.327179	57.957850
2528.738348	127651.045270	57.962855
2528.418351	127486.665591	57.967860
2527.285048	127325.362237	57.972865
2526.774984	127154.664583	57.977869
2526.439561	126991.750819	57.982874
2525.539952	126838.325398	57.987879
2525.005389	126667.190163	57.992884
2524.278631	126515.504438	57.997889
2523.556279	126347.131424	58.002893
2523.031923	126184.341308	58.007898
2522.279638	126016.876752	58.012903
2521.494406	125858.638273	58.017908
2520.860595	125698.903584	58.022913
2520.575963	125535.457080	58.027917
2519.408156	125378.336081	58.032922
2518.920384	125210.237704	58.037927
2518.579176	125044.860147	58.042932
2517.570356	124892.326545	58.047937
2516.947804	124723.706494	58.052941
2516.188885	124560.722014	58.057946
2515.146172	124398.837500	58.062951
2514.665825	124237.677544	58.067956
2514.313682	124078.872881	58.072961
2513.850457	123921.204236	58.077965
2512.806147	123774.295364	58.082970
2512.288161	123611.951466	58.087975
2511.983381	123438.374809	58.092980
2511.170776	123282.276401	58.097985
2510.599710	123115.220169	58.102989
2509.414199	122948.135390	58.107994
2509.147168	122778.734713	58.112999
2508.725140	122611.899271	58.118004
2507.622405	122454.035888	58.123009
2507.368112	122278.490598	58.128013
2506.603865	122116.791623	58.133018
2505.478560	121962.477405	58.138023
2505.029948	121794.622798	58.143028
2504.479671	121635.559333	58.148033
2503.630834	121465.573584	58.153037
2503.309178	121307.593227	58.158042
2502.764236	121147.973169	58.163047
2502.126641	120972.852813	58.168052
2501.150950	120814.166460	58.173057
2500.790851	120641.823077	58.178061
2499.964846	120474.849293	58.183066
2498.814714	120310.670467	58.188071
2498.505174	120141.242632	58.193076
2497.709395	119989.223950	58.198081
2497.279792	119813.278468	58.203085
2496.343672	119660.433270	58.208090
2495.441353	119493.319136	58.213095
2495.103563	119331.030089	58.218100
2494.415083	119178.611880	58.223105
2493.919210	119007.316489	58.228109
2493.271630	118849.281998	58.233114
2492.394072	118693.519429	58.238119
2492.298368	118526.283653	58.243124
2491.471082	118360.720164	58.248129
2490.791650	118188.367426	58.253133
2489.938763	118032.814402	58.258138
2489.046980	117861.709945	58.263143
2488.772853	117691.886188	58.268148
2488.052189	117540.092109	58.273153
2487.439093	117358.657116	58.278157
2487.081778	117202.205348	58.283162
2486.179504	117032.009436	58.288167
2485.842063	116862.353531	58.293172
2484.971226	116683.350853	58.298177
2484.000737	116516.381032	58.303181
2483.381723	116360.223435	58.308186
2482.915233	116185.178090	58.313191
2482.293821	116020.771309	58.318196
2481.203732	115856.649342	58.323201
2480.782447	115686.989136	58.328205
2480.158933	115522.655723	58.333210
2479.288548	115353.049891	58.338215
2478.734223	115184.048850	58.343220
2478.345817	115020.297093	58.348225
2477.503530	114857.589445	58.353229
2476.948713	114683.088901	58.358234
2476.061513	114520.847525	58.363239
2475.746020	114349.288090	58.368244
2474.980464	114184.897014	58.373249
2474.514796	114011.167650	58.378253
2473.980666	113844.780924	58.383258
2472.808927	113668.043213	58.388263
2471.999958	113499.982357	58.393268
2471.572725	113333.759778	58.398273
2470.744736	113161.985036	58.403277
2470.311051	112994.280613	58.408282
2469.718462	112833.882021	58.413287
2469.258893	112656.581600	58.418292
2468.109899	112489.266855	58.423297
2467.638148	112319.795977	58.428301
2467.266427	112151.484477	58.433306
2466.175112	111981.301775	58.438311
2465.805487	111809.197137	58.443316
2464.702251	111648.334996	58.448321
2464.420774	111476.618505	58.453325
2463.605945	111308.141803	58.458330
2462.824175	111139.654662	58.463335
2462.490639	110968.590904	58.468340
2461.690242	110815.821866	58.473345
2460.979127	110639.813200	58.478349
2460.803435	110472.433930	58.483354
2459.683456	110301.340817	58.488359
2459.173983	110125.246750	58.493364
2458.584557	109953.266027	58.498369
2457.988890	109783.235657	58.503373
2457.242032	109615.108774	58.508378
2456.517281	109433.520302	58.513383
2456.066342	109258.882685	58.518388
2455.287055	109094.851119	58.523393
2454.654318	108922.814696	58.528397
2454.043854	108747.076514	58.533402
2453.144868	108576.683812	58.538407
2452.600999	108399.560611	58.543412
2451.644741	108241.489480	58.548417
2451.262566	108062.826550	58.553421
2450.504750	107895.728513	58.558426
2449.639655	107727.220952	58.563431
2449.176176	107554.107723	58.568436
2448.549394	107384.993696	58.573441
2447.944175	107210.122406	58.578445
2447.319055	107030.991646	58.583450
2446.459376	106867.457415	58.588455
2445.938527	106692.430567	58.593460
2445.258457	106522.734603	58.598465
2444.753391	106356.343164	58.603469
2443.897625	106183.156032	58.608474
2443.028044	106015.892046	58.613479
2442.748219	105838.022462	58.618484
2441.935510	105673.461063	58.623489
2441.192264	105498.776377	58.628493
2440.683156	105314.760977	58.633498
2439.914294	105154.497855	58.638503
2439.135465	104984.314538	58.643508
2438.166638	104821.680776	58.648513
2437.838448	104650.159508	58.653517
2437.006012	104476.746307	58.658522
2436.628353	104311.979417	58.663527
2435.956498	104142.438634	58.668532
2435.429145	103975.470959	58.673537
2434.829646	103800.807673	58.678541
2434.020962	103636.494464	58.683546
2433.523760	103458.271097	58.688551
2432.792741	103281.418399	58.693556
2431.737818	103123.548974	58.698561
2431.184329	102949.284366	58.703565
2430.482965	102780.081583	58.708570
2429.851115	102610.678679	58.713575
2429.532424	102436.697840	58.718580
2428.449790	102268.929455	58.723585
2428.071746	102095.410966	58.728589
2427.610924	101928.434565	58.733594
2427.075442	101755.076775	58.738599
2426.275203	101568.669017	58.743604
2425.429251	101407.733080	58.748609
2424.786572	101231.008708	58.753613
2424.283570	101057.263996	58.758618
2423.310182	100881.089500	58.763623
2422.692313	100707.460762	58.768628
2422.080190	100539.522382	58.773633
2421.589221	100365.711154	58.778637
2421.115037	100200.880597	58.783642
2420.115616	100022.274600	58.788647
2419.754302	99842.852042	58.793652
2418.956987	99670.864335	58.798657
2418.246775	99502.676273	58.803661
2417.265567	99322.163545	58.808666
2416.612269	99152.218348	58.813671
2416.034104	98982.306894	58.818676
2415.198524	98815.158595	58.823681
2414.551633	98627.392824	58.828685
2414.140731	98478.091752	58.833690
2413.578610	98305.163606	58.838695
2413.258928	98125.887367	58.843700
2412.091878	97965.514704	58.848705
2411.523004	97784.067075	58.853709
2410.810864	97603.233456	58.858714
2410.355914	97444.996804	58.863719
2409.613206	97271.077630	58.868724
2408.636972	97107.541242	58.873729
2408.392660	96923.575471	58.878733
2407.464127	96754.719180	58.883738
2407.155371	96582.068355	58.888743
2406.575729	96408.218720	58.893748
2405.723971	96234.413562	58.898753
2405.163122	96058.375592	58.903757
2404.436951	95881.350476	58.908762
2403.532129	95712.276227	58.913767
2402.980314	95526.322086	58.918772
2402.611223	95353.778985	58.923777
2401.884466	95190.178846	58.928781
2401.132679	95016.341849	58.933786
2400.439779	94828.982587	58.938791
2399.980279	94653.313683	58.943796
2399.241719	94490.735179	58.948801
2398.551178	94306.075112	58.953805
2398.074958	94124.477263	58.958810
2397.579871	93951.451246	58.963815
2396.614185	93769.591443	58.968820
2395.794356	93600.697184	58.973825
2395.627337	93417.901918	58.978829
2394.677539	93240.768214	58.983834
2393.998834	93071.373654	58.988839
2393.709807	92870.776969	58.993844
2392.572344	92705.288018	58.998849
2392.030144	92522.369360	59.003853
2391.233135	92327.083192	59.008858
2390.619400	92153.107109	59.013863
2390.119606	91978.511939	59.018868
2389.200895	91802.513481	59.023873
2388.698831	91623.235561	59.028877
2387.738737	91448.032756	59.033882
2387.077845	91271.731343	59.038887
2386.680939	91096.391313	59.043892
2385.960697	90931.838646	59.048897
2385.142360	90743.290957	59.053901
2384.839543	90566.760885	59.058906
2384.093213	90397.346831	59.063911
2383.187882	90216.787453	59.068916
2382.814372	90034.794740	59.073921
2382.451358	89842.530550	59.078925
2381.461557	89677.396012	59.083930
2380.757210	89500.697272	59.088935
2380.352941	89301.527202	59.093940
2379.489958	89133.155876	59.098945
2378.873084	88949.657471	59.103949
2378.127164	88774.055371	59.108954
2377.241991	88601.805252	59.113959
2376.835802	88413.072865	59.118964
2376.072615	88233.008248	59.123969
2375.236105	88052.722182	59.128973
2374.622664	87887.199230	59.133978
2373.647961	87708.047408	59.138983
2373.464968	87531.396153	59.143988
2372.776747	87350.357037	59.148993
2371.945820	87173.532509	59.153997
2371.128788	86995.052622	59.159002
2370.384887	86826.477506	59.164007
2369.782884	86654.299457	59.169012
2368.877197	86480.712894	59.174017
2368.587045	86299.461025	59.179021
2367.887098	86131.233063	59.184026
2367.056291	85966.165070	59.189031
2366.735821	85788.332818	59.194036
2365.931445	85622.629373	59.199041
2365.337797	85444.710176	59.204045
2364.964885	85272.551291	59.209050
2363.969388	85093.766911	59.214055
2363.751121	84919.317022	59.219060
2362.892537	84739.474334	59.224065
2362.325447	84558.864329	59.229069
2361.564140	84376.733670	59.234074
2360.744353	84201.294798	59.239079
2360.334409	84007.727361	59.244084
2359.849503	83840.820847	59.249089
2359.079552	83659.306230	59.254093
2358.653915	83471.393793	59.259098
2357.724457	83303.947183	59.264103
2357.286623	83108.883863	59.269108
2356.402582	82934.549555	59.274113
2355.804995	82746.423654	59.279117
2355.138050	82563.964081	59.284122
2354.119734	82388.622472	59.289127
2353.573552	82205.170798	59.294132
2352.950776	82025.846242	59.299137
2352.426738	81843.870975	59.304141
2351.753605	81672.695363	59.309146
2350.861253	81500.389750	59.314151
2350.593216	81311.983629	59.319156
2349.488464	81131.355197	59.324161
2348.981037	80946.748614	59.329165
2348.416255	80767.761560	59.334170
2347.627935	80598.571357	59.339175
2347.199085	80402.473458	59.344180
2346.382725	80230.762028	59.349185
2345.273154	80048.743189	59.354189
2344.725705	79876.662505	59.359194
2344.028612	79708.098834	59.364199
2343.982266	79529.604270	59.369204
2343.071410	79353.542399	59.374209
2342.227412	79168.105135	59.379213
2341.683178	78991.804437	59.384218
2340.891449	78815.348044	59.389223
2340.866978	78635.603008	59.394228
2339.693987	78452.220506	59.399233
2338.884769	78277.900701	59.404237
2338.611098	78095.589114	59.409242
2337.756821	77916.400183	59.414247
2337.381369	77731.997828	59.419252
2336.551024	77560.329876	59.424257
2335.927254	77367.035522	59.429261
2335.185244	77186.586871	59.434266
2334.019434	77011.795789	59.439271
2333.816012	76830.605885	59.444276
2333.026669	76651.873966	59.449281
2332.481336	76471.685590	59.454285
2331.585541	76292.954696	59.459290
2331.012780	76117.449960	59.464295
2330.646738	75937.586376	59.469300
2329.543360	75763.303016	59.474305
2329.164074	75572.255250	59.479309
2328.316965	75398.574328	59.484314
2327.911844	75224.172207	59.489319
2327.230951	75048.110976	59.494324
2326.693768	74868.125634	59.499329
2325.908928	74684.525446	59.504333
2325.266457	74498.408092	59.509338
2324.628000	74320.591496	59.514343
2324.297745	74137.183969	59.519348
2323.161633	73962.579232	59.524353
2322.534424	73778.993986	59.529357
2321.762097	73594.609831	59.534362
2321.205432	73418.555828	59.539367
2320.991078	73238.977347	59.544372
2320.175710	73061.060591	59.549377
2319.467704	72867.391817	59.554381
2318.756158	72689.721644	59.559386
2318.131054	72505.488895	59.564391
2317.620711	72314.917320	59.569396
2316.838524	72134.900340	59.574401
2316.135984	71957.989121	59.579405
2315.851020	71759.766255	59.584410
2314.886301	71578.155216	59.589415
2314.345347	71391.480554	59.594420
2313.627741	71208.668124	59.599425
2312.912868	71016.095353	59.604429
2312.211776	70832.029535	59.609434
2311.236387	70654.755137	59.614439
2310.903149	70467.815536	59.619444
2309.986122	70296.521116	59.624449
2309.488514	70109.845344	59.629453
2308.947445	69932.141175	59.634458
2308.249932	69748.319268	59.639463
2308.003242	69552.779145	59.644468
2306.879660	69366.317381	59.649473
2306.158494	69180.224282	59.654477
2305.444919	69002.638219	59.659482
2304.777463	68817.065767	59.664487
2304.494730	68628.647182	59.669492
2303.542257	68450.508637	59.674497
2302.733132	68260.834322	59.679501
2302.267947	68085.719003	59.684506
2301.298332	67896.080021	59.689511
2300.626907	67718.435611	59.694516
2299.971713	67541.208257	59.699521
2299.571540	67353.865630	59.704525
2298.975944	67178.228149	59.709530
2298.146751	66998.386003	59.714535
2297.660525	66803.931051	59.719540
2296.911213	66628.702918	59.724545
2296.248470	66437.946536	59.729549
2295.553621	66254.590951	59.734554
2294.696847	66089.077474	59.739559
2294.493611	65889.637599	59.744564
2293.357925	65711.721071	59.749569
2292.903735	65525.639610	59.754573
2292.372718	65344.090544	59.759578
2291.472326	65165.951761	59.764583
2291.343114	64979.368088	59.769588
2290.660030	64797.610825	59.774593
2289.467333	64615.511829	59.779597
2288.931081	64428.171677	59.784602
2288.408512	64233.229167	59.789607
2287.836563	64053.734657	59.794612
2286.659832	63876.864321	59.799617
2286.420658	63674.410497	59.804621
2285.781749	63503.268111	59.809626
2284.902200	63326.130958	59.814631
2284.336920	63130.937359	59.819636
2283.422961	62960.331039	59.824641
2283.118059	62773.736597	59.829645
2282.349774	62587.413765	59.834650
2281.951686	62403.275495	59.839655
2281.146178	62223.993566	59.844660
2280.208917	62047.488497	59.849665
2279.883155	61853.770641	59.854669
2278.883500	61663.704134	59.859674
2278.122748	61497.259157	59.864679
2277.643225	61302.175251	59.869684
2276.987304	61126.267306	59.874689
2276.138578	60945.655783	59.879693
2275.607730	60755.236003	59.884698
2275.068488	60574.414345	59.889703
2274.488780	60384.917748	59.894708
2273.337259	60226.304738	59.899713
2272.792878	60029.541258	59.904718
2272.563870	59843.618985	59.909722
2271.685010	59666.224820	59.914727
2271.239373	59478.586882	59.919732
2270.414997	59301.143221	59.924737
2269.954646	59117.686353	59.929742
2269.226292	58942.244023	59.934746
2268.460161	58753.436063	59.939751
2268.064905	58572.595074	59.944756
2267.001835	58390.668476	59.949761
2266.686440	58197.562777	59.954766
2266.344023	58019.782668	59.959770
2265.366348	57832.843891	59.964775
2264.834107	57643.997436	59.969780
2264.344230	57451.579175	59.974785
2263.505461	57262.908657	59.979790
2262.730750	57069.042495	59.984794
2261.880651	56879.434521	59.989799
2261.487119	56687.901435	59.994804
2260.786632	56506.565648	59.999809
2260.408173	56322.192942	60.004814
2259.248513	56135.518568	60.009818
2258.610077	55946.415141	60.014823
2258.020199	55766.224248	60.019828
2257.659072	55571.229054	60.024833
2256.800924	55389.505208	60.029838
2256.208587	55199.310339	60.034842
2255.462142	55012.683108	60.039847
2254.934098	54807.560883	60.044852
2254.348563	54633.943795	60.049857
2253.454987	54444.083035	60.054862
2253.284427	54242.790159	60.059866
2252.314067	54066.815496	60.064871
2251.704804	53864.817916	60.069876
2250.726233	53679.437281	60.074881
2250.232310	53480.760943	60.079886
2249.610868	53298.485581	60.084890
2248.583742	53121.098791	60.089895
2248.419655	52925.012075	60.094900
2247.598055	52737.382184	60.099905
2246.971700	52540.081945	60.104910
2246.459989	52354.017449	60.109914
2245.580208	52159.599815	60.114919
2244.891615	51971.026517	60.119924
2244.298064	51789.024541	60.124929
2243.692604	51588.209768	60.129934
2242.813257	51411.911060	60.134938
2241.998582	51219.477060	60.139943
2241.507378	51028.620074	60.144948
2240.915461	50849.794429	60.149953
2240.214036	50666.966651	60.154958
2239.725467	50470.255687	60.159962
2238.938765	50282.329432	60.164967
2238.144831	50093.501456	60.169972
2237.429511	49906.140468	60.174977
2236.784320	49722.481345	60.179982
2236.045891	49518.297183	60.184986
2235.009838	49340.259393	60.189991
2235.196228	49153.573159	60.194996
2234.224695	48982.118501	60.200001
2233.388906	48788.666838	60.205006
2233.074337	48601.366707	60.210010
2232.257611	48417.776706	60.215015
2231.631924	48228.979747	60.220020
2230.955515	48043.950969	60.225025
2230.265633	47853.105651	60.230030
2229.652729	47656.201874	60.235034
2228.687353	47479.240731	60.240039
2228.104072	47286.818771	60.245044
2227.351666	47109.527036	60.250049
2226.687874	46921.041085	60.255054
2226.293674	46734.494530	60.260058
2225.236126	46550.437016	60.265063
2224.673444	46374.308754	60.270068
2223.740882	46199.540952	60.275073
2223.688928	46007.924836	60.280078
2222.890110	45824.795439	60.285082
2222.139038	45649.286318	60.290087
2221.747780	45457.062644	60.295092
2220.918299	45272.941219	60.300097
2220.016046	45089.778974	60.305102
2219.615290	44908.212240	60.310106
2219.131254	44716.659792	60.315111
2218.480789	44528.048761	60.320116
2217.532463	44347.890423	60.325121
2216.961527	44162.471424	60.330126
2216.212519	43979.527394	60.335130
2215.524897	43792.277517	60.340135
2215.243162	43604.671146	60.345140
2213.924495	43429.154195	60.350145
2213.097842	43237.716633	60.355150
2212.471587	43064.323127	60.360154
2211.862267	42887.136857	60.365159
2211.385567	42700.766597	60.370164
2210.795206	42520.472388	60.375169
2210.249770	42333.326385	60.380174
2209.442425	42150.777727	60.385178
2208.755382	41991.448583	60.390183
2208.459042	41792.277435	60.395188
2207.645724	41610.054834	60.400193
2207.087821	41427.458450	60.405198
2206.227876	41248.447230	60.410202
2205.798608	41069.571930	60.415207
2205.153640	40869.638272	60.420212
2204.125461	40692.604226	60.425217
2203.586165	40508.076303	60.430222
2203.145475	40330.911687	60.435226
2202.143818	40151.817389	60.440231
2201.766673	39950.830638	60.445236
2201.108728	39774.343375	60.450241
2200.368045	39587.076428	60.455246
2199.690929	39413.419486	60.460250
2199.242630	39224.703112	60.465255
2198.518135	39023.545237	60.470260
2197.684413	38861.737446	60.475265
2197.515464	38663.834483	60.480270
2196.844999	38473.884343	60.485274
2195.996243	38299.277969	60.490279
2195.342957	38108.295338	60.495284
2194.682415	37916.446577	60.500289
2194.141853	37726.420961	60.505294
2193.194388	37540.908664	60.510298
2192.398949	37353.006353	60.515303
2191.738285	37154.501896	60.520308
2191.407374	36979.700517	60.525313
2190.562865	36793.103643	60.530318
2189.985720	36597.965640	60.535322
2189.374549	36420.040558	60.540327
2188.624117	36226.437537	60.545332
2187.919992	36044.487938	60.550337
2187.354874	35852.381946	60.555342
2186.691300	35658.961348	60.560346
2186.048476	35481.566482	60.565351
2185.657154	35291.544629	60.570356
2184.810183	35111.246272	60.575361
2184.114061	34909.091323	60.580366
2183.472766	34715.041141	60.585370
2182.674932	34531.504412	60.590375
2181.665021	34347.094589	60.595380
2181.069679	34170.238700	60.600385
2180.711406	33983.252987	60.605390
2179.579408	33791.526088	60.610394
2179.144514	33608.243795	60.615399
2178.559655	33421.147041	60.620404
2178.122597	33243.024241	60.625409
2177.342930	33060.746141	60.630414
2176.882267	32860.950739	60.635418
2175.961512	32673.288316	60.640423
2175.655174	32485.069105	60.645428
2174.886155	32302.920906	60.650433
2174.058479	32117.866908	60.655438
2173.710689	31927.527295	60.660442
2172.523544	31745.788156	60.665447
2172.280264	31550.085762	60.670452
2171.433761	31377.354229	60.675457
2170.767993	31182.420077	60.680462
2170.049591	30987.318026	60.685466
2169.444816	30812.996060	60.690471
2168.831771	30611.872594	60.695476
2167.957516	30442.520869	60.700481
2167.237741	30247.656926	60.705486
2166.689774	30064.706793	60.710490
2165.919246	29883.694775	60.715495
2165.651772	29689.091196	60.720500
2164.733971	29500.845094	60.725505
2164.067731	29327.920088	60.730510
2163.363919	29137.629763	60.735514
2162.666328	28947.286951	60.740519
2162.322756	28764.360012	60.745524
2161.608532	28584.870161	60.750529
2160.630492	28388.053413	60.755534
2160.129208	28202.479915	60.760538
2159.568574	28037.533278	60.765543
2159.050707	27831.517199	60.770548
2158.096681	27648.922401	60.775553
2157.736112	27468.049097	60.780558
2156.773988	27267.150182	60.785562
2156.103238	27078.659094	60.790567
2155.839400	26888.584362	60.795572
2154.767744	26710.704280	60.800577
2154.258067	26518.537921	60.805582
2153.515855	26335.964612	60.810586
2152.635615	26154.017906	60.815591
2152.184781	25967.605041	60.820596
2151.616412	25772.617477	60.825601
2150.769455	25597.077139	60.830606
2150.110532	25413.824204	60.835610
2149.269795	25227.003162	60.840615
2148.492041	25042.773446	60.845620
2147.794179	24848.000079	60.850625
2147.248704	24678.915387	60.855630
2146.785221	24492.354208	60.860634
2145.761872	24325.689084	60.865639
2145.050393	24133.470311	60.870644
2144.697284	23976.330868	60.875649
2143.868302	23783.624785	60.880654
2143.381694	23593.422183	60.885658
2142.609897	23421.457687	60.890663
2142.048772	23241.793776	60.895668
2140.908432	23073.299004	60.900673
2140.384606	22888.323377	60.905678
2140.063925	22705.172576	60.910682
2139.175829	22541.539299	60.915687
2138.567528	22359.102216	60.920692
2137.719818	22185.480401	60.925697
2136.910886	22009.292794	60.930702
2136.365377	21838.475003	60.935706
2135.536301	21661.614599	60.940711
2135.075878	21495.469376	60.945716
2134.244241	21317.510156	60.950721
2133.872721	21143.385991	60.955726
2133.209413	20971.308448	60.960730
2132.463039	20796.514071	60.965735
2131.912533	20616.451069	60.970740
2130.802493	20450.264373	60.975745
2130.130973	20285.042567	60.980750
2129.382818	20114.226234	60.985754
2128.235182	19950.738339	60.990759
2127.783969	19787.541533	60.995764
2126.898137	19626.866399	61.000769
2126.327566	19463.519787	61.005774
2125.754046	19309.636969	61.010778
2124.923153	19163.114989	61.015783
2124.451462	18990.399106	61.020788
2123.450606	18846.134559	61.025793
2122.575499	18687.987327	61.030798
2121.728735	18540.580030	61.035802
2120.569830	18405.515278	61.040807
2119.803947	18251.671415	61.045812
2118.475511	18130.716320	61.050817
2117.988353	18006.443750	61.055822
2117.172160	17888.909556	61.060826
2116.114404	17770.411238	61.065831
2115.432792	17645.579948	61.070836
2114.475243	17535.670059	61.075841
2113.685377	17433.202400	61.080846
2112.904158	17320.762094	61.085850
2112.011211	17214.103220	61.090855
2111.595509	17108.920477	61.095860
2110.309602	17024.136567	61.100865
2109.455220	16923.978400	61.105870
2109.171732	16829.422981	61.110874
2107.900964	16742.956865	61.115879
2107.404664	16651.951511	61.120884
2106.469018	16572.603667	61.125889
2105.731554	16485.050711	61.130894
2105.033627	16414.984185	61.135898
2104.576302	16337.332934	61.140903
2103.787440	16250.915845	61.145908
2103.021991	16181.450724	61.150913
2102.400575	16109.056958	61.155918
2101.724612	16023.835235	61.160922
2100.992467	15962.588977	61.165927
2100.541857	15879.779377	61.170932
2099.797367	15799.805686	61.175937
2099.069529	15735.170347	61.180942
2098.597572	15661.625858	61.185946
2097.794269	15587.161289	61.190951
2097.433788	15516.328019	61.195956
2096.462397	15454.434266	61.200961
2095.761274	15375.560314	61.205966
2094.985236	15304.115567	61.210970
2094.326168	15246.398730	61.215975
2093.331385	15164.446111	61.220980
2092.796954	15111.337739	61.225985
2092.261607	15037.156815	61.230990
2091.604746	14979.237196	61.235994
2090.827067	14920.925562	61.240999
2090.302320	14855.657014	61.246004
2089.568146	14791.967838	61.251009
2089.213044	14733.613734	61.256014
2088.752243	14660.696953	61.261018
2087.982465	14601.671695	61.266023
2087.506501	14534.889598	61.271028
2086.521731	14465.925378	61.276033
2085.945251	14402.318456	61.281038
2085.494567	14333.434735	61.286042
2084.740516	14264.337833	61.291047
2084.506460	14200.431663	61.296052
2083.423135	14127.958428	61.301057
2082.377886	14066.441785	61.306062
2081.993417	14004.571657	61.311066
2081.342179	13938.212411	61.316071
2080.702486	13872.460301	61.321076
2079.785738	13812.195808	61.326081
2079.562237	13739.800563	61.331086
2078.598347	13688.582118	61.336090
2077.902235	13619.112153	61.341095
2077.517379	13560.968874	61.346100
2077.053918	13507.123510	61.351105
2076.355313	13437.075500	61.356110
2075.808883	13361.076680	61.361114
2075.128250	13291.886796	61.366119
2074.260012	13233.052118	61.371124
2073.474580	13172.921105	61.376129
2073.037567	13115.836414	61.381134
2072.676788	13045.567708	61.386138
2071.615065	12987.932060	61.391143
2071.161223	12912.058393	61.396148
2070.350072	12847.251855	61.401153
2069.466059	12779.300630	61.406158
2068.879216	12721.532925	61.411162
2068.472216	12664.541436	61.416167
2067.788164	12599.967224	61.421172
2067.014458	12537.727198	61.426177
2066.565100	12465.067449	61.431182
2065.978362	12395.305854	61.436186
2065.152596	12333.977103	61.441191
2064.883889	12266.485086	61.446196
2064.279940	12202.225957	61.451201
2063.451135	12133.664780	61.456206
2062.872736	12058.778056	61.461210
2061.827979	11998.640090	61.466215
2061.596607	11929.490052	61.471220
2060.878208	11867.105113	61.476225
2059.865139	11798.279763	61.481230
2059.294665	11731.373813	61.486234
2058.391590	11671.209927	61.491239
2058.115671	11597.201511	61.496244
2057.553308	11542.348726	61.501249
2056.828331	11479.982402	61.506254
2056.146337	11406.147071	61.511258
2055.189632	11336.819328	61.516263
2054.806289	11270.254215	61.521268
2053.798791	11218.013682	61.526273
2053.353808	11153.147880	61.531278
2053.148003	11082.715993	61.536282
2052.004972	11018.138103	61.541287
2051.635075	10951.177134	61.546292
2050.480579	10892.137655	61.551297
2049.608695	10838.455425	61.556302
2049.040845	10773.258635	61.561306
2048.415132	10721.504465	61.566311
2047.856252	10656.447995	61.571316
2047.099815	10600.663238	61.576321
2046.651682	10536.862827	61.581326
2045.977560	10465.530909	61.586330
2044.960148	10424.047679	61.591335
2044.486526	10360.828840	61.596340
2043.836923	10292.909756	61.601345
2043.062264	10230.460409	61.606350
2042.703286	10179.432698	61.611354
2042.068061	10124.672761	61.616359
2041.629368	10049.717388	61.621364
2040.616958	10000.083234	61.626369
2040.329487	9938.652926	61.631374
2039.885233	9870.884427	61.636378
2038.757905	9821.363387	61.641383
2038.398473	9749.210510	61.646388
2037.609871	9677.374623	61.651393
2036.859727	9618.382087	61.656398
2036.069322	9559.895996	61.661402
2035.216576	9498.570213	61.666407
2035.258717	9429.249133	61.671412
2034.255598	9369.355680	61.676417
2033.564036	9297.727514	61.681422
2033.459424	9232.455190	61.686426
2032.397517	9173.710727	61.691431
2031.921402	9111.223774	61.696436
2031.315477	9049.574257	61.701441
2030.210363	8989.583714	61.706446
2029.975464	8919.639913	61.711450
2029.158037	8851.640557	61.716455
2028.552244	8794.800330	61.721460
2027.823227	8741.300545	61.726465
2027.037698	8684.241928	61.731470
2026.492371	8617.506938	61.736474
2025.422809	8545.499367	61.741479
2025.140165	8476.186101	61.746484
2024.458012	8417.196964	61.751489
2023.632778	8351.724110	61.756494
2022.943381	8286.881238	61.761498
2021.948986	8244.474591	61.766503
2021.600982	8180.030839	61.771508
2020.786349	8117.233726	61.776513
2020.039077	8052.167934	61.781518
2019.447130	7994.372390	61.786522
2018.967068	7936.693821	61.791527
2018.674983	7869.236022	61.796532
2017.692850	7815.159254	61.801537
2017.113656	7748.035913	61.806542
2016.407949	7691.121463	61.811546
2015.470867	7633.669644	61.816551
2015.214048	7560.189619	61.821556
2014.603950	7502.489187	61.826561
2013.470804	7450.263180	61.831566
2013.286025	7379.892619	61.836570
2012.325963	7326.736314	61.841575
2011.760669	7263.534423	61.846580
2010.763796	7208.794814	61.851585
2010.312849	7140.729300	61.856590
2009.991052	7085.271633	61.861594
2009.145067	7034.542938	61.866599
2008.743444	6967.208362	61.871604
2008.146108	6905.186098	61.876609
2006.966812	6845.641929	61.881614
2006.250869	6783.742335	61.886618
2005.754360	6722.373769	61.891623
2005.356622	6659.149426	61.896628
2004.388328	6602.339978	61.901633
2003.865611	6540.159092	61.906638
2003.147787	6483.005858	61.911642
2002.113232	6431.209530	61.916647
2001.935006	6353.434146	61.921652
2001.085089	6313.730713	61.926657
2000.373548	6255.811415	61.931662
1999.720149	6197.728508	61.936666
1999.209320	6133.778134	61.941671
1998.503567	6073.965489	61.946676
1997.885594	6019.588982	61.951681
1997.300143	5945.248552	61.956686
1997.008385	5894.214135	61.961690
1995.708020	5828.700004	61.966695
1995.422545	5769.398487	61.971700
1994.512305	5716.402534	61.976705
1993.883085	5655.401774	61.981710
1993.322844	5595.269806	61.986714
1992.653057	5536.507430	61.991719
1992.153512	5479.820347	61.996724
1991.161628	5428.350463	62.001729
1990.758227	5358.812142	62.006734
1990.274513	5290.621482	62.011738
1989.029156	5238.509424	62.016743
1988.751505	5176.730752	62.021748
1988.316363	5117.263144	62.026753
1987.393560	5049.708036	62.031758
1986.455014	4997.285478	62.036762
1985.778842	4942.639006	62.041767
1985.433188	4874.170433	62.046772
1984.295198	4821.560098	62.051777
1983.770296	4766.558997	62.056782
1983.319398	4708.544441	62.061786
1982.386161	4649.369158	62.066791
1982.102538	4594.169501	62.071796
1981.481073	4545.827988	62.076801
1980.560042	4486.259427	62.081806
1980.108621	4419.703465	62.086810
1979.222737	4366.127213	62.091815
1978.899612	4304.077836	62.096820
1978.135407	4248.207270	62.101825
1977.515397	4190.208187	62.106830
1976.800602	4125.572474	62.111834
1975.813216	4076.190349	62.116839
1975.157888	4006.882147	62.121844
1974.425871	3963.995776	62.126849
1973.542182	3908.399425	62.131854
1972.999424	3853.711366	62.136858
1972.293850	3807.560826	62.141863
1971.791834	3744.766925	62.146868
1971.395207	3701.221589	62.151873
1970.489114	3644.690478	62.156878
1970.434937	3583.530505	62.161882
1969.450031	3527.969800	62.166887
1968.843596	3480.015853	62.171892
1968.240000	3419.035260	62.176897
1967.479132	3356.333004	62.181902
1966.587861	3304.814359	62.186906
1965.949751	3242.530808	62.191911
1965.373871	3184.464020	62.196916
1964.674325	3136.101683	62.201921
1964.091305	3078.885820	62.206926
1963.841376	3008.857091	62.211930
1962.640884	2953.356447	62.216935
1962.188586	2905.684325	62.221940
1961.403960	2844.745897	62.226945
1960.823245	2793.411613	62.231950
1960.330328	2738.719007	62.236954
1959.572265	2681.811654	62.241959
1958.858335	2622.875494	62.246964
1957.964674	2568.210862	62.251969
1957.227461	2512.773206	62.256974
1956.778120	2451.297408	62.261978
1956.238063	2403.222888	62.266983
1955.350708	2348.383007	62.271988
1954.538416	2285.790496	62.276993
1953.797050	2242.284502	62.281998
1953.566281	2188.141426	62.287002
1952.879005	2139.361692	62.292007
1952.033710	2075.683118	62.297012
1950.911724	2032.922665	62.302017
1950.703137	1974.477475	62.307022
1949.883161	1924.195190	62.312026
1949.113460	1887.508108	62.317031
1948.553784	1833.054233	62.322036
1947.897855	1781.076194	62.327041
1947.758485	1736.196292	62.332046
1946.864267	1678.129240	62.337050
1945.753049	1633.456760	62.342055
1945.306520	1570.900729	62.347060
1944.499020	1528.568130	62.352065
1943.816999	1470.652744	62.357070
1943.826947	1418.948802	62.362074
1942.721440	1378.129083	62.367079
1942.176105	1318.818155	62.372084
1941.247470	1273.686462	62.377089
1940.780489	1220.327282	62.382094
1939.949383	1173.290278	62.387098
1939.317814	1121.244490	62.392103
1938.804385	1065.346270	62.397108
1938.070785	1030.153840	62.402113
1937.279563	970.705944	62.407118
1936.749429	921.433015	62.412122
1935.877211	875.021710	62.417127
1935.325412	826.796550	62.422132
1934.729175	782.954894	62.427137
1933.838726	732.399320	62.432142
1933.166698	686.852594	62.437146
1932.387254	647.000360	62.442151
1931.869873	595.263197	62.447156
1930.831221	556.133635	62.452161
1930.268374	517.824389	62.457166
1929.754109	465.118909	62.462170
1928.972432	430.549024	62.467175
1928.550507	380.665434	62.472180
1927.728267	349.604695	62.477185
1927.118080	303.891656	62.482190
1926.182387	252.163776	62.487194
1925.280781	221.093835	62.492199
1924.903555	175.173906	62.497204
1924.238963	147.097447	62.502209
1923.711862	115.745927	62.507214
1922.936463	80.444170	62.512218
1922.093922	47.163783	62.517223
1921.185211	12.566180	62.522228
1919.683673	-15.605753	62.527233
1919.030566	-27.392162	62.532238
1916.927869	-22.761007	62.537242
1914.448921	29.143986	62.542247
1914.404108	25.521085	62.547252
1914.861174	31.728124	62.552257
1914.309522	33.891126	62.557262
1914.152574	28.171322	62.562266
1913.086832	40.264058	62.567271
1912.819526	32.876001	62.572276
1912.018798	39.159721	62.577281
1911.477869	36.932340	62.582286
1911.280067	40.147772	62.587290
1910.226439	47.004658	62.592295
1909.532514	42.915520	62.597300
1909.037184	46.392655	62.602305
1907.870551	46.894980	62.607310
1907.123302	36.998477	62.612314
1906.657656	50.348985	62.617319
1906.575198	43.322664	62.622324
1905.720672	42.061285	62.627329
1904.810077	47.245964	62.632334
1904.318141	51.837473	62.637338
1903.444712	51.820164	62.642343
1903.080064	38.656956	62.647348
1902.795313	46.512997	62.652353
1902.335140	46.606700	62.657358
1901.025138	38.848013	62.662362
1900.305054	51.406281	62.667367
1900.423469	42.868881	62.672372
1899.387422	49.377625	62.677377
1897.965053	54.889564	62.682382
1897.974966	53.099861	62.687386
1897.172060	60.938824	62.692391
1896.915158	52.164535	62.697396
1896.066093	53.933212	62.702401
1895.484989	59.705834	62.707406
1894.927795	48.571200	62.712410
1893.951338	59.564832	62.717415
1893.239348	51.189226	62.722420
1892.810565	54.239482	62.727425
1892.104514	60.552339	62.732430
1891.421298	49.716836	62.737434
1890.679755	58.722470	62.742439
1890.056618	52.822783	62.747444
1889.156540	55.309194	62.752449
1888.310711	52.243971	62.757454
1888.057143	48.411356	62.762458
1887.229976	58.203296	62.767463
1886.369637	59.073322	62.772468
1885.594383	59.382632	62.777473
1885.560513	56.015033	62.782478
1885.272993	53.790001	62.787482
1884.052112	58.899372	62.792487
1883.260057	49.793734	62.797492
1882.588644	49.799551	62.802497
1882.648064	57.108944	62.807502
1881.940321	51.730474	62.812506
1880.846358	59.593572	62.817511
1880.708456	46.257168	62.822516
1879.925808	51.585546	62.827521
1878.865827	59.695564	62.832526
1878.520708	53.176148	62.837530
1877.692094	62.752279	62.842535
1877.502604	55.936915	62.847540
1876.247545	56.860151	62.852545
1874.907077	60.115082	62.857550
1875.214403	54.395677	62.862554
1874.447464	54.035039	62.867559
1874.007912	50.436960	62.872564
1872.597532	54.986638	62.877569
1872.138413	48.024852	62.882574
1871.985533	43.690551	62.887578
1870.914145	52.352738	62.892583
1870.184548	44.664341	62.897588
1869.551465	52.725503	62.902593
1869.318620	51.187233	62.907598
1868.150187	41.827548	62.912602
1867.520242	61.344839	62.917607
1866.982900	49.579430	62.922612
1866.729035	49.993623	62.927617
1866.163810	48.083924	62.932622
1865.554808	54.572187	62.937626
1864.361069	57.437972	62.942631
1864.022148	49.056761	62.947636
1863.263396	48.843061	62.952641
1862.819801	48.308085	62.957646
1862.204695	53.475824	62.962650
1860.820339	52.412124	62.967655
1859.977583	46.815401	62.972660
1859.806356	47.874066	62.977665
1859.521905	48.551737	62.982670
1858.720724	47.876417	62.987674
1857.240212	59.869458	62.992679
1856.810910	53.902734	62.997684
1857.030648	50.018628	63.002689
1856.086258	53.305296	63.007694
1855.644309	45.951281	63.012698
1854.828447	51.978801	63.017703
1854.072718	42.898949	63.022708
1853.790391	50.343022	63.027713
1852.850326	45.241149	63.032718
1851.714284	49.922320	63.037722
1850.867397	53.783293	63.042727
1850.267185	47.050498	63.047732
1850.359272	45.954227	63.052737
1849.469784	52.706225	63.057742
1848.793258	49.489555	63.062746
1847.836816	52.432785	63.067751
1847.401134	51.817707	63.072756
1846.764573	53.465925	63.077761
1846.242515	49.806835	63.082766
1845.738065	48.748511	63.087770
1844.939700	58.871780	63.092775
1844.116306	57.717441	63.097780
1843.296131	52.317412	63.102785
1842.804251	56.520990	63.107790
1842.354357	47.562891	63.112794
1841.676038	51.474371	63.117799
1841.408100	56.462411	63.122804
1840.430605	52.140773	63.127809
1839.313319	50.355008	63.132814
1838.563248	47.776073	63.137818
1837.644288	53.826276	63.142823
1837.275746	46.824886	63.147828
1836.723950	52.152889	63.152833
1836.164127	50.336957	63.157838
1835.765114	52.762747	63.162842
1835.096791	60.261807	63.167847
1834.768203	48.789695	63.172852
1834.327048	48.429379	63.177857
1833.403437	50.981046	63.182862
1832.684804	38.186304	63.187866
1831.964318	57.476692	63.192871
1830.978128	44.628235	63.197876
1830.071211	45.584521	63.202881
1829.049709	47.645528	63.207886
1828.637834	45.299902	63.212890
1827.806721	50.380520	63.217895
1827.215163	51.237847	63.222900
1826.928836	46.137835	63.227905
1826.697689	50.229050	63.232910
1825.944627	45.433387	63.237914
1825.405548	53.979526	63.242919
1825.093804	43.801007	63.247924
1824.141507	55.030514	63.252929
1823.209260	56.441837	63.257934
1822.629111	46.269667	63.262938
1821.617730	53.627657	63.267943
1821.547726	39.643397	63.272948
1819.730035	56.788303	63.277953
1818.924186	57.920934	63.282958
1819.500897	49.903698	63.287962
1818.327723	55.823963	63.292967
1817.740061	50.215134	63.297972
1817.191638	59.887133	63.302977
1816.661583	59.170351	63.307982
1816.464760	51.137172	63.312986
1815.326265	56.861119	63.317991
1814.472233	43.228437	63.322996
1813.343466	42.333913	63.328001
1812.825131	47.544640	63.333006
1812.223576	50.565570	63.338010
1811.696530	40.958988	63.343015
1811.560773	45.030324	63.348020
1811.365922	54.572058	63.353025
1809.869964	46.497595	63.358030
1809.100168	41.660442	63.363034
1808.321251	44.422529	63.368039
1807.905151	48.569921	63.373044
1807.195013	52.369767	63.378049
1806.716690	56.146995	63.383054
1806.490695	42.518667	63.388058
1805.074685	52.875637	63.393063
1804.407313	53.547888	63.398068
1803.894934	51.650312	63.403073
1803.479229	50.860181	63.408078
1803.244026	40.606437	63.413082
1801.759243	51.225065	63.418087
1800.745379	40.153526	63.423092
1800.470636	43.737574	63.428097
1799.901419	47.655391	63.433102
1799.471233	37.066758	63.438106
1798.672142	52.417766	63.443111
1798.535773	48.717941	63.448116
1797.642237	55.243514	63.453121
1796.605649	51.251402	63.458126
1795.739913	47.429279	63.463130
1795.286354	52.971925	63.468135
1794.808118	36.753291	63.473140
1794.145736	43.011917	63.478145
1793.562148	44.459345	63.483150
1793.083021	40.807645	63.488154
1791.802482	53.447046	63.493159
1791.329429	39.356484	63.498164
1790.403073	42.753849	63.503169
1789.798184	37.895248	63.508174
1789.974754	35.129754	63.513178
1789.229395	46.354786	63.518183
1788.518369	47.906032	63.523188
1787.478499	57.703385	63.528193
1786.729680	46.171863	63.533198
1786.237296	43.963610	63.538202
1785.751972	47.871261	63.543207
1784.641228	44.296211	63.548212
1783.713690	43.324012	63.553217
1782.638002	41.448089	63.558222
1782.693356	34.926605	63.563226
1781.889135	42.627021	63.568231
1781.705125	32.688433	63.573236
1781.551089	40.840684	63.578241
1780.694639	49.238529	63.583246
1779.924171	48.772823	63.588250
1779.027365	54.827410	63.593255
1778.508751	42.593860	63.598260
1777.865767	48.215473	63.603265
1776.423290	45.563589	63.608270
1775.981731	37.375324	63.613274
1775.140672	46.784708	63.618279
1774.641630	44.140697	63.623284
1774.194176	48.628965	63.628289
1773.722907	51.846832	63.633294
1773.445721	46.136672	63.638298
1772.966586	45.091690	63.643303
1772.036947	44.928810	63.648308
1771.412196	50.984347	63.653313
1770.647922	47.436281	63.658318
1769.491280	51.329122	63.663322
1768.542654	48.218766	63.668327
1767.954838	46.893000	63.673332
1767.406636	40.956222	63.678337
1767.090185	44.955329	63.683342
1767.175274	43.797089	63.688346
1765.643814	46.024262	63.693351
1764.968153	47.708669	63.698356
1764.289504	47.698320	63.703361
1763.609470	44.811818	63.708366
1763.281498	49.470347	63.713370
1762.630840	45.036914	63.718375
1761.991390	37.941373	63.723380
1760.821375	44.151314	63.728385
1759.973873	52.252852	63.733390
1759.896950	40.712412	63.738394
1759.316713	43.520230	63.743399
1758.902727	44.059210	63.748404
1757.728025	49.938737	63.753409
1756.642969	61.310775	63.758414
1755.908318	40.390955	63.763418
1755.287369	55.732604	63.768423
1755.438072	42.296777	63.773428
1754.571991	44.359936	63.778433
1754.432126	41.043873	63.783438
1753.491411	42.284675	63.788442
1752.633663	50.414649	63.793447
1751.639482	47.404576	63.798452
1751.299831	54.862488	63.803457
1750.506851	47.043851	63.808462
1749.651927	39.094707	63.813466
1748.684948	45.321293	63.818471
1748.584555	45.698506	63.823476
1748.237852	51.402382	63.828481
1747.621899	38.061510	63.833486
1746.906478	44.096756	63.838490
1745.692465	49.312324	63.843495
1745.423405	31.374724	63.848500
1744.764201	41.258279	63.853505
1744.010790	51.968936	63.858510
1743.582559	41.791592	63.863514
1742.171232	46.000858	63.868519
1741.814764	41.627942	63.873524
1741.366000	37.674964	63.878529
1740.742281	47.349459	63.883534
1740.473274	44.907042	63.888538
1739.253083	45.250791	63.893543
1738.539107	46.048731	63.898548
1737.809914	46.879051	63.903553
1737.135653	49.132525	63.908558
1736.613768	43.336656	63.913562
1736.201209	53.017043	63.918567
1735.488363	40.923168	63.923572
1734.473085	45.165731	63.928577
1733.927644	49.557602	63.933582
1733.491418	37.227408	63.938586
1733.022628	43.740728	63.943591
1732.089521	36.781724	63.948596
1731.080019	39.779150	63.953601
1730.257574	38.812357	63.958606
1730.114472	37.326083	63.963610
1729.545696	41.002566	63.968615
1729.270751	35.763572	63.973620
1728.253940	46.131284	63.978625
1727.366545	47.754712	63.983630
1726.801855	41.522519	63.988634
1726.439540	46.068233	63.993639
1725.977182	49.716779	63.998644
1724.834286	43.292568	64.003649
1723.877888	45.567201	64.008654
1723.584937	45.222789	64.013658
1722.690180	49.332675	64.018663
1722.055892	42.783529	64.023668
1720.800244	44.192634	64.028673
1720.323613	50.825476	64.033678
1719.800143	48.770407	64.038682
1719.411701	53.099499	64.043687
1718.905819	34.358999	64.048692
1718.614992	43.881275	64.053697
1717.924635	41.411166	64.058702
1717.003836	38.359492	64.063706
1716.264941	47.213343	64.068711
1715.627518	42.345736	64.073716
1715.096857	40.634012	64.078721
1714.395747	44.525483	64.083726
1713.929596	42.779859	64.088730
1713.068396	50.278031	64.093735
1712.529022	45.603009	64.098740
1711.689006	44.664244	64.103745
1710.715785	48.915906	64.108750
1710.635463	40.703396	64.113754
1709.538313	47.918922	64.118759
1709.155848	43.234749	64.123764
1708.027949	41.051759	64.128769
1707.403344	39.222494	64.133774
1706.600028	44.950010	64.138778
1706.339544	45.250151	64.143783
1705.779113	48.871698	64.148788
1705.607977	53.186777	64.153793
1704.309609	46.738383	64.158798
1703.641980	50.384843	64.163802
1702.674288	51.943762	64.168807
1702.381925	49.531867	64.173812
1702.088321	51.489921	64.178817
1700.945775	46.073342	64.183822
1700.621975	50.852639	64.188826
1699.644139	49.144136	64.193831
1699.203127	39.872433	64.198836
1698.420373	43.761106	64.203841
1696.934352	46.089910	64.208846
1696.578770	41.171234	64.213850
1695.739275	53.898310	64.218855
1695.911527	37.589006	64.223860
1695.579744	39.548392	64.228865
1694.849968	46.574682	64.233870
1694.279746	39.591170	64.238874
1693.366436	48.447498	64.243879
1692.653254	50.259309	64.248884
1692.307350	35.047872	64.253889
1690.865431	38.473543	64.258894
1690.388602	44.936106	64.263898
1689.629468	43.599724	64.268903
1689.329346	32.451147	64.273908
1688.928552	38.201460	64.278913
1687.987555	42.395970	64.283918
1687.481491	40.904272	64.288922
1686.498787	44.222312	64.293927
1685.735233	48.991036	64.298932
1684.782000	52.469977	64.303937
1683.930157	48.547918	64.308942
1683.749521	44.274816	64.313946
1683.031143	47.189747	64.318951
1682.661652	44.110438	64.323956
1682.295430	41.680317	64.328961
1681.489641	48.259790	64.333966
1680.785893	41.469379	64.338970
1679.764776	44.575902	64.343975
1679.405159	43.969271	64.348980
1678.940315	41.663626	64.353985
1677.698031	47.044561	64.358990
1676.925555	43.007397	64.363994
1676.159824	53.019854	64.368999
1675.920103	39.365356	64.374004
1676.117100	46.499903	64.379009
1675.336357	49.401089	64.384014
1674.571522	43.760523	64.389018
1672.861315	49.576911	64.394023
1671.977155	44.959822	64.399028
1672.098280	41.375227	64.404033
1671.020374	44.769896	64.409038
1670.811283	35.111278	64.414042
1669.918538	49.742316	64.419047
1669.803850	44.490488	64.424052
1668.955816	41.777357	64.429057
1667.856744	48.660465	64.434062
1667.335885	37.346680	64.439066
1666.623755	39.008518	64.444071
1666.556621	32.629501	64.449076
1665.431665	33.968985	64.454081
1664.597086	40.769075	64.459086
1663.920677	33.119620	64.464090
1663.547376	43.355165	64.469095
1662.806235	29.904909	64.474100
1661.371849	42.899946	64.479105
1660.569599	46.164097	64.484110
1660.812020	32.341557	64.489114
1659.768371	46.167085	64.494119
1659.426661	50.231715	64.499124
1659.139127	45.616050	64.504129
1658.942524	41.946309	64.509134
1657.938913	37.430204	64.514138
1656.814006	45.020741	64.519143
1656.397590	42.231166	64.524148
1655.093678	48.604345	64.529153
1654.392822	49.450686	64.534158
1653.852632	32.046617	64.539162
1653.376989	36.900497	64.544167
1653.161107	35.706488	64.549172
1652.733796	40.732465	64.554177
1651.751810	47.060813	64.559182
1651.273868	30.526801	64.564186
1650.457953	41.520209	64.569191
1649.208763	35.352623	64.574196
1648.712098	42.846515	64.579201
1647.961502	44.462429	64.584206
1647.572230	39.151722	64.589210
1647.250243	38.258421	64.594215
1646.722682	36.593529	64.599220
1645.665403	37.639995	64.604225
1644.427472	48.064936	64.609230
1644.321547	33.923994	64.614234
1643.807760	40.018692	64.619239
1643.002130	41.091415	64.624244
1641.995280	33.568578	64.629249
1641.479602	42.541522	64.634254
1641.389894	38.662413	64.639258
1640.581568	36.999547	64.644263
1639.533301	41.253689	64.649268
1638.625434	38.043873	64.654273
1638.114296	41.400556	64.659278
1637.945201	30.305295	64.664282
1637.195572	37.385209	64.669287
1636.669016	32.389629	64.674292
1635.833186	36.988494	64.679297
1635.099761	43.168548	64.684302
1634.845528	27.978844	64.689306
1633.380890	36.239944	64.694311
1632.508416	36.060147	64.699316
1632.342321	37.223664	64.704321
1631.495657	29.044604	64.709326
1631.664870	31.534689	64.714330
1630.320821	39.361895	64.719335
1629.464188	37.599474	64.724340
1628.886842	34.971090	64.729345
1628.326293	44.212939	64.734350
1628.356663	36.280902	64.739354
1627.136470	36.230464	64.744359
1626.523705	28.821650	64.749364
1625.788415	31.059611	64.754369
1625.246645	33.009786	64.759374
1625.182109	35.164844	64.764378
1623.480113	40.640908	64.769383
1622.932078	35.927865	64.774388
1622.630774	33.011201	64.779393
1621.484239	38.348560	64.784398
1621.154313	33.405325	64.789402
1620.352122	40.036277	64.794407
1619.993306	32.227573	64.799412
1619.747957	39.689426	64.804417
1618.647588	32.947857	64.809422
1617.828638	32.032586	64.814426
1616.545381	47.449493	64.819431
1616.405755	36.519861	64.824436
1616.074236	35.252763	64.829441
1615.691616	32.434175	64.834446
1614.650388	31.901148	64.839450
1614.130271	37.799736	64.844455
1613.525926	32.644632	64.849460
1612.902828	34.142528	64.854465
1611.836814	33.261779	64.859470
1611.900154	31.960336	64.864474
1610.361660	39.930407	64.869479
1609.405632	29.759689	64.874484
1609.238848	31.385364	64.879489
1608.478942	39.343704	64.884494
1608.340291	37.520840	64.889498
1607.646049	34.917341	64.894503
1606.318416	29.410372	64.899508
1605.720617	36.152356	64.904513
1605.045513	39.393168	64.909518
1604.941021	35.565297	64.914522
1604.258817	32.158794	64.919527
1603.533530	39.936594	64.924532
1602.752839	36.526813	64.929537
1602.218423	34.311086	64.934542
1601.871463	39.078297	64.939546
1600.608712	33.592561	64.944551
1600.219242	31.268651	64.949556
1599.509814	40.542039	64.954561
1598.490904	41.196074	64.959566
1597.893808	38.217597	64.964570
1597.055459	50.089796	64.969575
1596.553637	37.694371	64.974580
1596.279502	32.248690	64.979585
1595.417403	35.973375	64.984590
1594.986757	34.504410	64.989594
1593.768595	46.736571	64.994599
1593.462495	41.854208	64.999604
1592.852646	38.956607	65.004609
1592.189512	38.454982	65.009614
1591.516218	37.808314	65.014618
1590.738191	44.765020	65.019623
1590.179984	40.737998	65.024628
1590.118462	35.862511	65.029633
1588.882396	37.358452	65.034638
1588.385482	30.005360	65.039642
1587.458466	43.875452	65.044647
1586.982182	35.115589	65.049652
1586.055708	43.204479	65.054657
1584.985964	48.283649	65.059662
1585.141776	35.555086	65.064666
1584.318303	44.897062	65.069671
1583.574525	36.081928	65.074676
1582.643545	39.218318	65.079681
1581.910503	37.775322	65.084686
1582.102494	35.505688	65.089690
1581.451369	51.079220	65.094695
1579.814154	33.185579	65.099700
1579.327874	30.907016	65.104705
1578.834537	38.081840	65.109710
1578.819320	38.902843	65.114714
1577.646680	39.570273	65.119719
1576.687741	36.636677	65.124724
1576.409350	37.699768	65.129729
1575.651271	41.912558	65.134734
1575.147358	42.126809	65.139738
1573.788892	44.015944	65.144743
1573.180815	47.887935	65.149748
1572.963515	41.569053	65.154753
1572.507128	40.039525	65.159758
1572.203934	33.313247	65.164762
1571.009311	38.152063	65.169767
1570.362269	32.697827	65.174772
1570.033550	36.055498	65.179777
1568.725993	38.590981	65.184782
1568.034129	35.168677	65.189786
1567.316019	39.190615	65.194791
1567.116289	41.078571	65.199796
1566.779682	37.128311	65.204801
1566.103001	44.284962	65.209806
1565.528648	40.626366	65.214810
1564.571625	38.022054	65.219815
1563.732829	34.085355	65.224820
1562.866508	36.429309	65.229825
1562.208704	37.390258	65.234830
1562.018775	33.763625	65.239834
1561.077959	45.803496	65.244839
1560.363749	30.915552	65.249844
1559.556536	37.597778	65.254849
1558.411100	33.965270	65.259854
1557.994522	29.378015	65.264858
1557.503547	33.707639	65.269863
1557.182005	39.912152	65.274868
1556.845677	37.441033	65.279873
1555.634738	35.498390	65.284878
1555.049876	31.664850	65.289882
1554.405351	39.291054	65.294887
1554.131728	24.495541	65.299892
1553.414823	39.852433	65.304897
1552.209623	41.690417	65.309902
1552.045241	30.455652	65.314906
1551.314109	44.387667	65.319911
1550.679822	35.283913	65.324916
1549.952277	34.467681	65.329921
1549.024846	41.265206	65.334926
1548.503684	29.844281	65.339930
1547.764074	33.650442	65.344935
1547.282769	31.462559	65.349940
1546.604808	31.997784	65.354945
1545.885889	41.763122	65.359950
1545.445211	32.726379	65.364954
1544.656049	43.264549	65.369959
1543.945744	34.398380	65.374964
1543.094260	32.471168	65.379969
1542.233225	36.941599	65.384974
1542.146761	28.868865	65.389978
1541.356914	37.986306	65.394983
1540.575514	37.421485	65.399988
1540.156695	32.582276	65.404993
1539.479521	46.272332	65.409998
1539.257729	33.788278	65.415002
1537.774451	32.637972	65.420007
1536.914480	33.681514	65.425012
1536.867765	33.756892	65.430017
1535.920409	41.663032	65.435022
1535.279182	25.158169	65.440026
1534.269912	32.421285	65.445031
1533.739190	26.868154	65.450036
1533.685228	41.031611	65.455041
1533.227530	35.466874	65.460046
1532.397886	29.136495	65.465050
1531.261643	37.392770	65.470055
1530.775748	35.409047	65.475060
1529.716785	41.569889	65.480065
1529.004519	35.170394	65.485070
1528.515648	31.491919	65.490074
1527.864951	36.223821	65.495079
1527.596169	31.575240	65.500084
1527.301212	39.863416	65.505089
1526.314323	43.754609	65.510094
1525.447808	30.582956	65.515098
1525.195900	38.905291	65.520103
1524.150382	31.595236	65.525108
1523.041914	37.021200	65.530113
1522.318301	43.515111	65.535118
1521.916669	45.655927	65.540122
1521.703190	39.885226	65.545127
1521.331081	37.069715	65.550132
1520.178828	40.510946	65.555137
1519.379926	29.356516	65.560142
1519.271125	37.127831	65.565146
1518.369142	46.690455	65.570151
1517.538174	40.013358	65.575156
1517.108658	38.436993	65.580161
1516.034515	43.518463	65.585166
1515.193955	32.752274	65.590170
1514.519405	41.405123	65.595175
1514.395006	42.366479	65.600180
1513.718338	35.590748	65.605185
1513.068645	44.496693	65.610190
1512.172151	35.860396	65.615194
1511.682787	38.611242	65.620199
1511.221258	30.883540	65.625204
1510.725843	34.729753	65.630209
1509.502754	32.535175	65.635214
1508.875066	34.850686	65.640218
1508.180590	42.669340	65.645223
1507.619143	42.809168	65.650228
1506.823738	37.648186	65.655233
1505.951138	39.472760	65.660238
1505.811182	39.783729	65.665242
1504.835395	45.101886	65.670247
1504.335403	36.033577	65.675252
1503.575981	36.655875	65.680257
1502.834073	46.787576	65.685262
1502.612805	35.465662	65.690266
1501.623991	44.400267	65.695271
1500.952662	34.600672	65.700276
1500.539454	37.596462	65.705281
1499.668117	47.507458	65.710286
1499.269205	40.654475	65.715290
1498.157174	39.970321	65.720295
1497.789727	36.400289	65.725300
1497.182600	36.224103	65.730305
1496.326518	39.829590	65.735310
1495.489502	36.301064	65.740314
1494.498271	39.032319	65.745319
1494.197769	36.564979	65.750324
1493.883181	34.935662	65.755329
1493.333104	44.652103	65.760334
1493.022910	35.747600	65.765338
1491.721213	44.780816	65.770343
1491.390109	44.574960	65.775348
1490.739637	40.527933	65.780353
1489.230391	37.252895	65.785358
1488.969370	34.006574	65.790362
1488.046693	40.423315	65.795367
1487.738623	40.123912	65.800372
1487.558612	43.369651	65.805377
1486.589948	38.087976	65.810382
1485.966243	40.737173	65.815386
1485.359548	38.119797	65.820391
1485.024807	35.992214	65.825396
1483.915758	40.281303	65.830401
1483.084225	42.227092	65.835406
1482.869425	29.852330	65.840410
1481.430092	37.576471	65.845415
1480.598815	30.459472	65.850420
1480.232455	42.086367	65.855425
1479.882804	40.823747	65.860430
1479.717364	45.615738	65.865434
1478.666313	48.447971	65.870439
1477.840669	37.791389	65.875444
1477.455654	37.933146	65.880449
1476.648323	38.058441	65.885454
1475.880014	30.628661	65.890458
1474.955610	32.959795	65.895463
1474.513663	35.505992	65.900468
1474.098229	34.537679	65.905473
1473.144394	36.127592	65.910478
1472.914868	37.392661	65.915482
1471.883929	40.269007	65.920487
1471.756313	39.329070	65.925492
1470.399503	40.224512	65.930497
1469.830429	45.315618	65.935502
1469.412566	32.517389	65.940506
1468.903610	40.331797	65.945511
1468.120287	35.837537	65.950516
1466.804304	35.184233	65.955521
1466.392702	40.868477	65.960526
1466.240109	38.644139	65.965530
1465.436591	43.028181	65.970535
1464.862376	37.923524	65.975540
1463.959160	36.837192	65.980545
1463.154416	45.583283	65.985550
1462.840280	32.815879	65.990554
1462.229485	44.639320	65.995559
1461.429786	38.302629	66.000564
1460.903026	48.909502	66.005569
1459.858517	48.255634	66.010574
1459.464826	39.255597	66.015578
1458.247258	44.905508	66.020583
1457.629420	48.794843	66.025588
1457.626678	36.946197	66.030593
1456.962605	39.458314	66.035598
1456.553438	32.179620	66.040602
1455.286435	43.199027	66.045607
1454.997116	35.718358	66.050612
1454.744348	43.668672	66.055617
1453.195072	45.731696	66.060622
1452.697120	46.899080	66.065626
1452.079935	40.517615	66.070631
1451.880460	39.161745	66.075636
1450.848822	32.773613	66.080641
1449.994464	37.922676	66.085646
1449.522825	43.338920	66.090650
1449.076279	39.311536	66.095655
1448.224559	37.994674	66.100660
1447.270010	38.449305	66.105665
1446.663149	40.066083	66.110670
1446.314751	37.032351	66.115674
1445.335240	47.999765	66.120679
1444.611846	47.312213	66.125684
1444.120035	43.569567	66.130689
1443.442520	50.396793	66.135694
1443.043355	36.099068	66.140698
1442.369485	41.137446	66.145703
1441.523725	40.791042	66.150708
1441.082707	37.742069	66.155713
1440.525133	44.222224	66.160718
1439.464235	41.923053	66.165722
1438.386347	40.536485	66.170727
1438.254590	44.674996	66.175732
1437.970642	43.395631	66.180737
1437.288789	44.418782	66.185742
1436.458359	37.659630	66.190746
1435.673238	39.892947	66.195751
1435.152979	35.826820	66.200756
1434.297239	38.244826	66.205761
1433.350693	41.003694	66.210766
1432.782097	37.523991	66.215770
1432.416956	40.658807	66.220775
1432.036654	36.333893	66.225780
1431.210357	35.782549	66.230785
1430.068921	38.860976	66.235790
1430.008617	38.463853	66.240794
1428.824487	47.248175	66.245799
1428.219900	38.087701	66.250804
1427.523424	35.255953	66.255809
1427.218244	35.747728	66.260814
1426.949698	35.385280	66.265818
1425.682566	43.279199	66.270823
1425.190254	41.638716	66.275828
1424.654983	31.189899	66.280833
1423.602625	39.734078	66.285838
1423.097411	30.948900	66.290842
1422.001000	32.358066	66.295847
1421.664294	40.891000	66.300852
1421.349062	34.896792	66.305857
1420.528854	33.287927	66.310862
1419.820513	32.345678	66.315866
1418.771434	32.250795	66.320871
1418.506696	31.733202	66.325876
1418.016610	39.178763	66.330881
1417.104134	42.023685	66.335886
1416.822016	39.279044	66.340890
1416.005119	38.902830	66.345895
1415.044202	33.815498	66.350900
1414.395014	28.984549	66.355905
1413.554586	44.413134	66.360910
1413.338256	30.177827	66.365914
1412.715612	35.438302	66.370919
1411.571510	41.544908	66.375924
1410.859581	38.034377	66.380929
1410.031982	43.992907	66.385934
1409.831286	35.263407	66.390938
1409.379524	51.751435	66.395943
1408.912817	33.757042	66.400948
1408.452896	32.805273	66.405953
1407.547842	31.331324	66.410958
1406.247167	35.048504	66.415962
1405.492420	44.297593	66.420967
1405.389343	39.179566	66.425972
1404.982389	40.576921	66.430977
1404.110292	44.464103	66.435982
1403.306375	24.534785	66.440986
1402.215349	40.373784	66.445991
1401.599281	27.673317	66.450996
1401.585886	36.320438	66.456001
1400.409806	41.342458	66.461006
1399.970278	34.371378	66.466010
1399.318306	36.969893	66.471015
1398.901338	33.076592	66.476020
1398.217486	27.483183	66.481025
1397.286024	30.108777	66.486030
1397.076267	37.621744	66.491034
1395.698741	40.578441	66.496039
1394.866859	35.155216	66.501044
1394.527404	29.945457	66.506049
1393.940006	37.188869	66.511054
1393.754043	29.767480	66.516058
1392.931514	33.783977	66.521063
1391.975658	35.549282	66.526068
1391.387442	39.082259	66.531073
1390.845407	34.112858	66.536078
1390.388357	35.111325	66.541082
1389.088470	38.498806	66.546087
1388.440330	26.054179	66.551092
1388.040748	38.708217	66.556097
1387.602740	38.186630	66.561102
1387.120243	32.435060	66.566106
1385.859598	19.870182	66.571111
1385.389362	34.041434	66.576116
1385.238626	35.968921	66.581121
1384.025173	37.603288	66.586126
1383.757876	25.542825	66.591130
1382.997560	33.477620	66.596135
1382.052309	32.315998	66.601140
1381.267336	33.546365	66.606145
1381.001602	29.059749	66.611150
1380.483683	26.103440	66.616154
1379.251568	38.692698	66.621159
1378.456179	36.483814	66.626164
1378.059377	28.206543	66.631169
1377.385825	31.995937	66.636174
1377.505912	33.333171	66.641178
1376.075361	38.703156	66.646183
1375.512890	38.094123	66.651188
1375.003846	22.965500	66.656193
1374.041382	39.274499	66.661198
1373.344495	33.750977	66.666202
1372.361998	30.147852	66.671207
1371.890915	28.289542	66.676212
1371.762630	36.573302	66.681217
1371.188598	39.228820	66.686222
1370.570203	30.266108	66.691226
1369.597120	37.879915	66.696231
1369.103037	39.844636	66.701236
1368.830023	35.248791	66.706241
1367.312028	42.882992	66.711246
1366.474513	33.836839	66.716250
1366.060410	36.927405	66.721255
1365.877433	37.454954	66.726260
1364.986475	31.180118	66.731265
1363.983426	36.458497	66.736270
1363.753236	31.551494	66.741274
1363.119754	36.807394	66.746279
1362.634386	33.052707	66.751284
1361.881683	32.109642	66.756289
1361.295695	35.561845	66.761294
1360.720203	24.977522	66.766298
1359.320367	38.694161	66.771303
1358.829796	41.599765	66.776308
1358.349307	38.544468	66.781313
1357.903662	41.665281	66.786318
1356.899524	33.773141	66.791322
1356.123178	33.319537	66.796327
1355.297411	31.405650	66.801332
1355.238604	33.756916	66.806337
1354.573209	35.904990	66.811342
1353.905051	32.313403	66.816346
1352.979908	36.984890	66.821351
1352.489458	25.466111	66.826356
1352.264063	26.978113	66.831361
1351.100080	37.886560	66.836366
1350.293725	29.571900	66.841370
1349.948963	39.396062	66.846375
1349.217611	34.759542	66.851380
1347.913357	34.172244	66.856385
1347.631831	39.433698	66.861390
1347.396394	23.277570	66.866394
1346.840289	33.680950	66.871399
1345.878692	30.970222	66.876404
1345.027547	30.359779	66.881409
1344.452366	31.198838	66.886414
1344.149750	40.495907	66.891418
1343.045240	35.874556	66.896423
1342.595991	33.359922	66.901428
1341.993855	34.092880	66.906433
1341.396348	29.676360	66.911438
1340.701900	31.879518	66.916442
1339.887515	39.546954	66.921447
1339.399633	37.861630	66.926452
1338.322211	32.597311	66.931457
1337.575263	36.787890	66.936462
1337.269145	34.655778	66.941466
1336.725225	44.036943	66.946471
1335.975896	31.367144	66.951476
1335.059598	38.954589	66.956481
1334.658604	34.735486	66.961486
1334.358008	29.833374	66.966490
1333.257587	39.615243	66.971495
1332.453680	32.713147	66.976500
1331.989237	29.067105	66.981505
1330.990017	36.350765	66.986510
1330.704574	27.117517	66.991514
1329.715592	32.556094	66.996519
1329.091078	31.904897	67.001524
1328.884965	34.047769	67.006529
1328.383070	31.312851	67.011534
1327.336975	33.945654	67.016538
1326.322225	31.918318	67.021543
1325.791855	27.658287	67.026548
1325.182455	29.578269	67.031553
1324.861818	42.038411	67.036558
1324.364421	34.371653	67.041562
1323.404260	28.478421	67.046567
1323.007984	30.195788	67.051572
1321.923569	30.134947	67.056577
1320.691574	28.429157	67.061582
1320.965123	28.644433	67.066586
1320.363032	31.933624	67.071591
1319.714233	33.389941	67.076596
1318.629430	30.853352	67.081601
1317.771536	39.480188	67.086606
1317.410450	36.306570	67.091610
1317.146757	38.220478	67.096615
1316.128252	28.343688	67.101620
1315.405274	34.250912	67.106625
1314.666036	33.151180	67.111630
1314.337117	30.893387	67.116634
1313.110161	39.651440	67.121639
1312.572019	32.972026	67.126644
1312.123492	36.959048	67.131649
1311.638069	37.900538	67.136654
1310.998532	31.592060	67.141658
1309.965137	35.656299	67.146663
1309.501197	31.983372	67.151668
1309.211253	31.501338	67.156673
1307.989875	33.736240	67.161678
1307.260043	32.097275	67.166682
1306.720857	32.618383	67.171687
1306.467237	34.814541	67.176692
1306.016423	32.369550	67.181697
1304.631468	29.951651	67.186702
1304.526461	29.116939	67.191706
1303.686239	44.605433	67.196711
1302.713759	34.637749	67.201716
1302.248548	30.446210	67.206721
1301.378359	45.444308	67.211726
1301.269541	24.327475	67.216730
1300.258349	38.294581	67.221735
1299.393620	28.905859	67.226740
1299.178770	28.842393	67.231745
1298.385830	27.341198	67.236750
1297.648330	25.607262	67.241754
1296.899161	29.151652	67.246759
1296.587654	29.737488	67.251764
1295.161917	27.829126	67.256769
1294.162593	30.085499	67.261774
1293.999186	17.235842	67.266778
1293.299630	38.703830	67.271783
1293.015599	34.898224	67.276788
1292.944887	28.026229	67.281793
1291.853899	28.974117	67.286798
1291.322946	24.558070	67.291802
1290.794489	30.631488	67.296807
1289.793904	21.817884	67.301812
1288.771520	28.050258	67.306817
1288.165391	30.223617	67.311822
1288.107503	31.844609	67.316826
1286.796868	29.386519	67.321831
1286.240420	33.228277	67.326836
1285.727888	33.814537	67.331841
1285.121574	31.324888	67.336846
1284.892763	28.251671	67.341850
1283.348057	29.970290	67.346855
1283.126536	22.680731	67.351860
1282.532059	27.709669	67.356865
1281.610856	31.472227	67.361870
1280.912375	22.866058	67.366874
1280.248731	32.206333	67.371879
1279.753287	16.241383	67.376884
1279.415607	24.280883	67.381889
1278.354324	36.215387	67.386894
1277.760713	34.999471	67.391898
1276.793321	29.386529	67.396903
1276.510839	32.591795	67.401908
1276.309647	28.016086	67.406913
1275.139009	31.356261	67.411918
1274.811569	31.963556	67.416922
1273.936254	35.755092	67.421927
1272.721790	33.567145	67.426932
1272.069401	34.598268	67.431937
1271.502933	38.201926	67.436942
1271.346127	35.244993	67.441946
1271.090032	34.464268	67.446951
1269.958690	31.059895	67.451956
1269.420146	30.828703	67.456961
1268.617144	27.460434	67.461966
1267.465736	22.233148	67.466970
1266.701163	32.612912	67.471975
1266.207824	27.181643	67.476980
1266.035684	29.476811	67.481985
1265.340648	27.557938	67.486990
1265.097166	24.431864	67.491994
1263.708985	29.383581	67.496999
1263.245742	36.676657	67.502004
1263.229630	34.564676	67.507009
1261.643574	39.131546	67.512014
1261.151135	30.502080	67.517018
1260.298632	28.395358	67.522023
1260.129551	28.548545	67.527028
1259.789661	36.287206	67.532033
1258.582478	34.421384	67.537038
1258.233187	29.736761	67.542042
1257.424510	32.585729	67.547047
1256.300007	28.912194	67.552052
1255.692165	28.933298	67.557057
1254.990761	33.638623	67.562062
1254.867095	23.296307	67.567066
1254.260532	33.174711	67.572071
1253.225984	29.701338	67.577076
1252.726414	26.959760	67.582081
1252.293949	37.294607	67.587086
1251.812760	24.076014	67.592090
1250.552001	30.921892	67.597095
1249.984771	37.053523	67.602100
1249.812866	28.480326	67.607105
1248.634607	35.642671	67.612110
1248.086419	31.541609	67.617114
1247.716141	39.469608	67.622119
1246.837889	29.983710	67.627124
1245.748427	26.066490	67.632129
1245.024596	36.919175	67.637134
1244.764977	24.187322	67.642138
1244.134627	27.376942	67.647143
1243.600435	23.183772	67.652148
1242.719503	22.141287	67.657153
1241.928159	34.215802	67.662158
1241.739939	28.669788	67.667162
1240.903673	28.191055	67.672167
1239.994059	19.153277	67.677172
1239.585930	20.583958	67.682177
1238.753403	25.622370	67.687182
1238.557686	15.938067	67.692186
1237.231165	18.415222	67.697191
1236.603775	20.891591	67.702196
1236.446558	22.339143	67.707201
1235.613414	25.860632	67.712206
1235.170960	23.502636	67.717210
1234.094326	31.296949	67.722215
1233.813565	30.165338	67.727220
1233.033904	21.513749	67.732225
1232.178346	23.677897	67.737230
1231.750218	20.093913	67.742234
1230.806771	28.302284	67.747239
1229.630943	11.560884	67.752244
1229.259698	21.026549	67.757249
1228.398818	28.808632	67.762254
1228.052610	17.710084	67.767258
1227.479549	19.173301	67.772263
1227.480583	11.555055	67.777268
1226.786158	18.925888	67.782273
1225.927832	16.039518	67.787278
1225.087030	11.415721	67.792282
1224.049585	23.204514	67.797287
1223.597704	15.341323	67.802292
1223.283510	21.489484	67.807297
1222.163522	26.278725	67.812302
1221.594090	24.139619	67.817306
1220.647137	22.260819	67.822311
1220.402494	19.775177	67.827316
1220.126426	23.356316	67.832321
1218.828288	17.201491	67.837326
1218.046592	19.823827	67.842330
1217.498878	26.351323	67.847335
1217.248656	18.064981	67.852340
1216.592771	23.546816	67.857345
1215.522186	24.876266	67.862350
1215.124304	19.570180	67.867354
1214.461871	26.928048	67.872359
1213.704980	22.388679	67.877364
1212.903382	21.726248	67.882369
1212.036671	20.514356	67.887374
1212.279528	15.442269	67.892378
1211.306759	21.772431	67.897383
1210.198085	23.828605	67.902388
1209.696387	19.587700	67.907393
1209.266930	24.325480	67.912398
1208.723805	23.331788	67.917402
1207.537126	23.936961	67.922407
1206.835653	21.675355	67.927412
1206.227569	18.671926	67.932417
1205.879403	22.406456	67.937422
1205.474569	17.755912	67.942426
1204.614216	19.383092	67.947431
1204.198833	10.260432	67.952436
1203.226681	21.941075	67.957441
1202.072719	26.989615	67.962446
1201.847527	14.304346	67.967450
1201.208536	21.581215	67.972455
1200.549572	15.102405	67.977460
1199.669762	12.154807	67.982465
1198.811271	13.494688	67.987470
1198.585568	17.091471	67.992474
1198.152665	17.180962	67.997479
1197.433893	18.883399	68.002484
1196.420719	20.870775	68.007489
1195.728814	20.317061	68.012494
1195.576812	12.693192	68.017498
1194.472215	24.262439	68.022503
1193.348118	18.890501	68.027508
1193.111736	23.181264	68.032513
1192.457350	27.185267	68.037518
1192.512584	11.845559	68.042522
1191.126703	16.273396	68.047527
1190.677566	18.677273	68.052532
1190.325860	20.393876	68.057537
1189.244687	30.013452	68.062542
1188.593480	11.868740	68.067546
1187.909389	21.855668	68.072551
1187.352497	18.290595	68.077556
1186.953098	11.068771	68.082561
1185.852321	16.332781	68.087566
1185.030413	17.548578	68.092570
1184.647778	15.315121	68.097575
1184.199668	20.533683	68.102580
1183.379207	18.953326	68.107585
1182.316718	25.143227	68.112590
1182.043648	19.956070	68.117594
1181.613564	20.193348	68.122599
1180.763643	19.256339	68.127604
1180.089480	17.979144	68.132609
1179.393828	23.847355	68.137614
1178.902600	23.750583	68.142618
1177.720948	18.367306	68.147623
1177.089803	15.164128	68.152628
1176.920875	21.438998	68.157633
1176.255445	20.595652	68.162638
1175.548913	17.562157	68.167642
1174.598009	17.189988	68.172647
1174.008561	27.078292	68.177652
1173.718123	14.138479	68.182657
1172.874529	22.906568	68.187662
1172.425654	16.943131	68.192666
1171.662102	17.887879	68.197671
1171.136077	17.866029	68.202676
1169.949192	21.131559	68.207681
1169.048025	21.703957	68.212686
1168.909958	15.948133	68.217690
1168.289891	24.535594	68.222695
1167.255161	27.273883	68.227700
1166.723164	23.307463	68.232705
1166.373081	30.716589	68.237710
1166.088871	17.042505	68.242714
1164.703164	22.847003	68.247719
1164.262357	22.677560	68.252724
1163.899931	22.762156	68.257729
1162.492762	27.026240	68.262734
1162.220866	25.079523	68.267738
1161.303669	26.461870	68.272743
1161.025650	27.599057	68.277748
1160.278346	18.896622	68.282753
1159.095334	22.633048	68.287758
1158.701370	19.698079	68.292762
1158.332956	16.483081	68.297767
1158.027855	23.951281	68.302772
1157.312287	18.014494	68.307777
1156.470024	26.156330	68.312782
1156.169933	15.501474	68.317786
1154.525159	20.397859	68.322791
1153.954735	20.185955	68.327796
1153.518889	13.171784	68.332801
1153.291504	25.626540	68.337806
1152.293591	15.517910	68.342810
1151.214751	20.811562	68.347815
1150.573917	11.399922	68.352820
1150.425589	9.443017	68.357825
1150.117252	18.740985	68.362830
1149.272935	12.088248	68.367834
1148.300988	12.883221	68.372839
1147.639090	12.476135	68.377844
1147.028924	25.419124	68.382849
1145.990502	27.793733	68.387854
1145.622056	20.959650	68.392858
1145.254244	19.983821	68.397863
1144.616007	13.497003	68.402868
1143.489068	21.725118	68.407873
1142.573877	27.694487	68.412878
1142.491267	14.805205	68.417882
1141.888884	23.426127	68.422887
1141.172378	23.995972	68.427892
1140.428440	17.795623	68.432897
1139.872539	21.697241	68.437902
1139.641144	21.048219	68.442906
1138.331347	30.609559	68.447911
1137.634807	26.364967	68.452916
1137.320051	16.303803	68.457921
1136.350514	25.350552	68.462926
1135.674564	24.010575	68.467930
1135.056757	21.341446	68.472935
1134.290750	24.459626	68.477940
1134.207898	20.002310	68.482945
1133.166604	24.395870	68.487950
1132.474752	21.765328	68.492954
1131.850543	26.958292	68.497959
1131.237572	20.087413	68.502964
1130.535168	19.825545	68.507969
1129.615394	29.149810	68.512974
1129.168636	20.194580	68.517978
1128.405115	16.496809	68.522983
1127.823088	32.789492	68.527988
1126.879140	24.236616	68.532993
1126.220220	25.049617	68.537998
1126.177287	22.084050	68.543002
1125.597196	23.064284	68.548007
1124.573598	17.476124	68.553012
1124.065924	18.425917	68.558017
1123.527286	26.016421	68.563022
1122.648653	20.170237	68.568026
1121.779200	27.070620	68.573031
1121.315369	21.715120	68.578036
1120.873442	19.735530	68.583041
1119.568092	30.882577	68.588046
1118.975486	25.460827	68.593050
1118.434737	21.407504	68.598055
1118.337608	23.104123	68.603060
1117.512110	30.369676	68.608065
1116.334646	24.395985	68.613070
1115.820237	20.106662	68.618074
1115.079824	26.742095	68.623079
1114.856747	32.144071	68.628084
1114.110725	26.838188	68.633089
1113.069821	30.250834	68.638094
1113.129112	26.075259	68.643098
1112.044763	33.982805	68.648103
1111.279281	35.259036	68.653108
1111.009778	23.645267	68.658113
1110.352987	25.684797	68.663118
1109.073440	21.432027	68.668122
1108.264144	27.157482	68.673127
1108.115626	21.221977	68.678132
1107.509180	30.649373	68.683137
1106.511545	27.439853	68.688142
1105.923593	18.150699	68.693146
1105.105362	24.431083	68.698151
1104.815902	27.583855	68.703156
1104.704221	27.180721	68.708161
1103.375890	33.723598	68.713166
1102.962171	28.125164	68.718170
1102.083299	27.799911	68.723175
1101.311073	22.649589	68.728180
1100.330806	26.650256	68.733185
1099.437016	27.886976	68.738190
1099.475753	28.204234	68.743194
1098.830939	36.962806	68.748199
1098.653872	25.354836	68.753204
1097.978015	19.197288	68.758209
1096.804448	24.922343	68.763214
1096.243312	18.434313	68.768218
1095.234738	25.727414	68.773223
1094.772770	24.501642	68.778228
1094.460544	24.389029	68.783233
1093.731911	28.838525	68.788238
1093.230049	19.295985	68.793242
1091.766236	36.131062	68.798247
1091.498460	29.392936	68.803252
1091.153194	19.877526	68.808257
1089.758712	34.539582	68.813262
1089.283383	22.608479	68.818266
1088.643996	28.792611	68.823271
1088.654442	26.745797	68.828276
1088.178142	18.769830	68.833281
1086.880779	27.575431	68.838286
1086.558832	19.917108	68.843290
1085.798177	22.148206	68.848295
1084.763525	27.562588	68.853300
1084.070397	22.278265	68.858305
1083.701223	22.996300	68.863310
1083.185633	17.584390	68.868314
1082.414834	24.062237	68.873319
1081.707630	21.539807	68.878324
1081.538294	23.650034	68.883329
1080.076865	25.909033	68.888334
1079.535907	18.687672	68.893338
1079.096872	29.875118	68.898343
1078.230642	30.448298	68.903348
1077.407426	25.325018	68.908353
1076.832068	21.304020	68.913358
1076.245061	24.404778	68.918362
1075.740491	27.736851	68.923367
1075.308714	29.183933	68.928372
1074.065654	28.371001	68.933377
1073.283517	32.901554	68.938382
1073.223505	31.063066	68.943386
1072.682928	31.358941	68.948391
1071.786988	28.071757	68.953396
1071.191440	24.323628	68.958401
1070.386305	40.806356	68.963406
1070.110946	18.987539	68.968410
1069.077463	27.145623	68.973415
1068.348794	25.657934	68.978420
1068.207775	25.152237	68.983425
1066.708097	31.687695	68.988430
1066.077783	18.089195	68.993434
1065.409199	28.409569	68.998439
1065.254273	32.256876	69.003444
1064.695200	24.697778	69.008449
1063.531674	29.883513	69.013454
1063.064516	22.435950	69.018458
1062.527705	33.191102	69.023463
1062.362063	21.688556	69.028468
1061.165481	24.340669	69.033473
1060.167720	22.452669	69.038478
1059.739397	18.121281	69.043482
1059.527563	23.344849	69.048487
1058.714878	21.018979	69.053492
1057.665048	23.105278	69.058497
1057.080586	26.809606	69.063502
1056.851726	18.195045	69.068506
1055.857967	23.918319	69.073511
1054.972724	26.886756	69.078516
1054.921125	23.462103	69.083521
1053.878162	30.672381	69.088526
1053.156109	22.998868	69.093530
1052.314029	28.106660	69.098535
1051.828821	29.486553	69.103540
1051.565221	24.594375	69.108545
1050.355324	34.556174	69.113550
1049.798202	20.417758	69.118554
1048.995101	33.385150	69.123559
1048.857564	26.396080	69.128564
1048.226055	31.454606	69.133569
1046.905607	36.788316	69.138574
1046.516714	23.562995	69.143578
1046.106991	28.893740	69.148583
1045.662333	21.510412	69.153588
1044.615730	28.147264	69.158593
1043.508189	33.611105	69.163598
1043.329763	24.792978	69.168602
1042.935083	24.687181	69.173607
1041.960005	35.079978	69.178612
1041.653874	25.295000	69.183617
1040.679462	29.737878	69.188622
1040.075247	19.509898	69.193626
1039.219373	23.342563	69.198631
1038.822844	26.056636	69.203636
1038.375279	30.545008	69.208641
1037.271801	26.830388	69.213646
1036.559489	16.917650	69.218650
1035.993170	24.851611	69.223655
1035.849497	29.655909	69.228660
1034.736910	32.343557	69.233665
1033.868386	33.101620	69.238670
1033.516497	23.316040	69.243674
1033.008201	25.718315	69.248679
1032.056090	24.950579	69.253684
1031.548388	23.364668	69.258689
1030.834965	28.803657	69.263694
1030.521376	23.545700	69.268698
1029.229429	31.158296	69.273703
1028.718476	26.463169	69.278708
1028.367773	23.571803	69.283713
1027.394006	29.656181	69.288718
1026.314378	27.714988	69.293722
1026.149944	29.933248	69.298727
1025.693808	25.177361	69.303732
1025.225244	21.295503	69.308737
1023.964647	24.829867	69.313742
1023.577269	21.174788	69.318746
1023.059270	19.137935	69.323751
1021.903757	30.672763	69.328756
1020.918432	25.236254	69.333761
1020.405609	38.283627	69.338766
1020.146752	24.439962	69.343770
1019.800282	29.408988	69.348775
1019.397778	27.019448	69.353780
1018.658903	25.915018	69.358785
1017.660524	28.527731	69.363790
1017.502720	23.192952	69.368794
1016.238733	25.158800	69.373799
1015.808475	14.680806	69.378804
1014.697575	21.870363	69.383809
1013.462353	27.349797	69.388814
1013.209344	23.241259	69.393818
1012.720834	24.260563	69.398823
1012.218650	24.949308	69.403828
1011.909249	28.270839	69.408833
1010.951630	28.021225	69.413838
1010.263142	25.562071	69.418842
1009.549750	24.929826	69.423847
1009.323755	31.912367	69.428852
1008.401836	29.608623	69.433857
1007.317645	24.900628	69.438862
1006.958131	21.819857	69.443866
1006.555028	35.873208	69.448871
1005.971192	34.624266	69.453876
1004.913529	25.042448	69.458881
1004.186388	32.901081	69.463886
1003.880865	21.086491	69.468890
1003.061894	18.879911	69.473895
1001.964328	34.500850	69.478900
1001.623845	16.227933	69.483905
1001.163300	34.374703	69.488910
1001.022186	23.593660	69.493914
999.539342	31.734956	69.498919
999.057375	23.532833	69.503924
998.737528	19.819707	69.508929
997.752666	35.604064	69.513934
997.182809	21.898199	69.518938
996.535641	31.849327	69.523943
995.699446	25.469742	69.528948
994.542545	22.738195	69.533953
993.920168	32.910883	69.538958
993.693599	35.228916	69.543962
993.491341	32.906866	69.548967
993.215847	27.634969	69.553972
992.221290	20.403804	69.558977
991.329135	30.133717	69.563982
990.558065	31.609567	69.568986
989.790505	25.296334	69.573991
989.060545	38.785110	69.578996
988.524684	21.293904	69.584001
987.900160	31.045889	69.589006
986.951768	23.881496	69.594010
986.225701	23.446816	69.599015
985.580925	26.135741	69.604020
985.552373	18.787146	69.609025
984.220252	26.622192	69.614030
983.693233	21.764056	69.619034
983.036131	20.244505	69.624039
982.862017	23.588666	69.629044
982.360957	23.357880	69.634049
981.319952	30.908491	69.639054
980.801695	15.887141	69.644058
979.660271	23.944156	69.649063
978.765267	20.781440	69.654068
978.599183	20.013234	69.659073
977.707310	27.592154	69.664078
977.634765	23.762410	69.669082
977.008603	23.070564	69.674087
975.915386	29.940360	69.679092
975.477456	20.758264	69.684097
974.614860	22.387452	69.689102
973.764944	22.144369	69.694106
973.212273	28.977040	69.699111
972.234254	27.240475	69.704116
972.264469	20.609500	69.709121
971.480774	30.233851	69.714126
970.694085	22.737809	69.719130
970.045992	24.373867	69.724135
969.415481	25.373197	69.729140
968.998080	24.115129	69.734145
967.270402	32.975062	69.739150
967.462374	16.465610	69.744154
966.846547	24.945195	69.749159
966.471993	21.294395	69.754164
965.639710	17.312733	69.759169
964.818710	26.574014	69.764174
964.184773	19.801141	69.769178
962.789432	27.802375	69.774183
962.692145	20.620835	69.779188
962.170067	22.019226	69.784193
961.593293	22.117457	69.789198
960.947929	25.874072	69.794202
959.889806	21.232916	69.799207
959.389476	26.831975	69.804212
959.106851	16.997550	69.809217
957.777634	29.487280	69.814222
957.142243	26.825729	69.819226
956.674936	26.348305	69.824231
956.175989	18.111053	69.829236
956.018327	23.811701	69.834241
954.878793	31.792736	69.839246
954.523848	20.143717	69.844250
953.654994	22.789459	69.849255
952.586423	29.112873	69.854260
952.054001	23.342553	69.859265
951.580709	25.152649	69.864270
951.109704	17.929657	69.869274
950.166672	29.025422	69.874279
949.520785	24.990449	69.879284
949.015183	24.400850	69.884289
948.034278	29.775189	69.889294
947.286859	24.253547	69.894298
946.739543	27.466287	69.899303
946.430780	15.809925	69.904308
945.900279	22.019331	69.909313
944.362320	26.690689	69.914318
944.106523	28.240674	69.919322
943.484155	31.317126	69.924327
943.164470	23.842973	69.929332
942.761287	17.873898	69.934337
941.606747	24.002838	69.939342
941.067355	18.339288	69.944346
940.254273	26.962230	69.949351
939.034248	30.852875	69.954356
939.001817	14.546294	69.959361
938.181834	24.362501	69.964366
937.943555	13.620592	69.969370
936.990506	20.226820	69.974375
936.486020	19.253850	69.979380
936.151144	13.163523	69.984385
934.968972	22.876518	69.989390
934.075517	15.954145	69.994394
933.348652	26.436775	69.999399
932.882651	17.916745	70.004404
932.789735	24.567447	70.009409
931.727805	23.550723	70.014414
930.724406	20.495161	70.019418
930.186979	25.534005	70.024423
930.038254	23.925683	70.029428
929.385982	13.003655	70.034433
928.156703	26.111420	70.039438
927.714076	14.999912	70.044442
927.102451	25.424780	70.049447
926.451863	20.635208	70.054452
925.645110	21.657864	70.059457
924.927393	17.727371	70.064462
924.632816	19.925344	70.069466
924.022501	27.148814	70.074471
923.085420	27.652897	70.079476
922.594126	24.094799	70.084481
921.773152	30.610632	70.089486
921.078974	25.078950	70.094490
920.144836	25.484795	70.099495
919.714028	19.398697	70.104500
919.350586	19.527643	70.109505
918.332397	29.119936	70.114510
917.607668	19.166642	70.119514
917.014729	27.954829	70.124519
916.654810	17.806286	70.129524
916.303616	24.140125	70.134529
915.079201	28.818373	70.139534
914.791465	16.351278	70.144538
914.166758	26.885463	70.149543
913.427675	20.772731	70.154548
912.616301	19.630987	70.159553
911.875166	18.495411	70.164558
911.254139	15.431045	70.169562
910.298991	27.353487	70.174567
909.494047	22.066517	70.179572
909.254589	22.470621	70.184577
908.572041	32.206622	70.189582
907.966065	19.971520	70.194586
907.322971	27.476174	70.199591
906.938321	26.378483	70.204596
906.230676	19.093815	70.209601
904.753581	23.787047	70.214606
904.409897	16.313572	70.219610
903.870661	24.866132	70.224615
903.577148	21.807992	70.229620
902.923877	29.296921	70.234625
901.785542	33.035811	70.239630
901.600612	15.802609	70.244634
900.950492	27.193965	70.249639
899.840515	21.397307	70.254644
899.310334	22.445341	70.259649
898.665844	26.559795	70.264654
897.799717	22.517312	70.269658
896.657493	26.644749	70.274663
896.215833	32.784834	70.279668
895.838462	24.417861	70.284673
895.307255	25.186941	70.289678
895.004194	18.683128	70.294682
894.840970	21.781133	70.299687
893.850813	24.438314	70.304692
893.299359	21.252494	70.309697
891.959773	25.053377	70.314702
891.274007	16.904223	70.319706
890.438307	19.415398	70.324711
890.001160	22.459227	70.329716
889.541200	23.571781	70.334721
888.175197	24.150448	70.339726
888.146844	17.155066	70.344730
887.193277	24.450517	70.349735
887.018243	21.949106	70.354740
886.695814	21.311445	70.359745
885.399734	19.914117	70.364750
885.109856	10.790490	70.369754
883.955235	18.397056	70.374759
882.938081	25.582781	70.379764
882.749895	26.932778	70.384769
882.199395	25.464097	70.389774
881.876392	17.052209	70.394778
880.663049	26.453222	70.399783
879.973288	25.681637	70.404788
880.027991	20.273631	70.409793
878.679932	25.356345	70.414798
878.079262	19.513332	70.419802
877.645911	23.669879	70.424807
876.960753	18.422205	70.429812
876.827233	19.225764	70.434817
875.062172	25.868211	70.439822
874.800496	17.347216	70.444826
874.260482	21.069735	70.449831
873.838179	23.969279	70.454836
872.966516	12.471914	70.459841
872.020937	20.196601	70.464846
872.043123	23.846987	70.469850
871.169061	19.096155	70.474855
870.139838	26.772657	70.479860
869.806780	17.559709	70.484865
868.992429	18.230357	70.489870
867.982020	18.455974	70.494874
867.084582	20.710480	70.499879
866.813217	20.708086	70.504884
866.727647	23.716461	70.509889
865.791198	23.239608	70.514894
864.917764	17.597707	70.519898
864.346574	23.463520	70.524903
863.763300	22.285487	70.529908
863.212845	20.864113	70.534913
862.023508	29.397150	70.539918
861.546857	18.213805	70.544922
861.222638	24.090772	70.549927
860.600574	21.092816	70.554932
859.731763	13.444315	70.559937
859.122385	24.633650	70.564942
858.687144	24.323028	70.569946
857.276341	28.308727	70.574951
856.255003	24.196347	70.579956
855.975642	20.880497	70.584961
855.555249	26.537810	70.589966
855.321439	22.238583	70.594970
855.118256	22.248992	70.599975
854.089680	20.471638	70.604980
853.283649	25.994790	70.609985
852.665050	21.512384	70.614990
851.649982	9.809200	70.619994
850.908037	24.007935	70.624999
850.595903	20.889689	70.630004
849.974354	15.330705	70.635009
848.899602	21.730829	70.640014
848.442793	15.186845	70.645018
848.386892	19.642859	70.650023
846.910639	14.730846	70.655028
846.034318	22.923907	70.660033
845.196374	22.451883	70.665038
845.120563	18.733055	70.670042
844.741733	26.400659	70.675047
843.893929	24.801115	70.680052
843.066703	14.293317	70.685057
842.695104	24.000329	70.690062
842.312164	21.825326	70.695066
841.200009	23.767091	70.700071
840.464812	19.169208	70.705076
840.098006	11.111231	70.710081
839.599163	18.829473	70.715086
838.775718	18.711532	70.720090
837.960900	19.751268	70.725095
837.184349	16.000479	70.730100
836.644262	18.822582	70.735105
835.715917	28.641870	70.740110
835.211490	16.398520	70.745114
834.888458	18.716147	70.750119
833.805703	21.345511	70.755124
832.815277	19.514786	70.760129
832.305801	21.740665	70.765134
832.109419	22.011765	70.770138
831.922713	22.462673	70.775143
830.941316	25.525334	70.780148
830.098575	17.002223	70.785153
829.306163	20.656115	70.790158
828.704981	17.158109	70.795162
828.017490	17.056378	70.800167
827.244569	23.350119	70.805172
827.064946	18.644884	70.810177
826.061638	17.856992	70.815182
825.551306	22.654998	70.820186
824.800260	21.795414	70.825191
824.000415	23.154467	70.830196
823.247199	23.123122	70.835201
822.286324	29.811059	70.840206
822.271855	14.788425	70.845210
821.633176	24.869109	70.850215
820.436899	21.587255	70.855220
819.952807	13.864917	70.860225
819.184886	16.980330	70.865230
819.201504	8.650017	70.870234
817.873966	26.210967	70.875239
817.412095	23.168600	70.880244
816.893905	20.754936	70.885249
816.173904	22.393016	70.890254
815.624099	22.133753	70.895258
814.588473	18.506212	70.900263
814.035001	26.286773	70.905268
813.800160	17.476093	70.910273
812.370168	32.072945	70.915278
812.119189	27.315989	70.920282
811.640417	18.380137	70.925287
811.175942	26.114992	70.930292
810.567287	13.041428	70.935297
809.340638	20.684719	70.940302
808.898884	18.736702	70.945306
808.014227	24.472653	70.950311
807.378793	26.027889	70.955316
806.794483	16.895951	70.960321
806.441835	24.002730	70.965326
805.810782	9.656991	70.970330
804.762498	19.140563	70.975335
803.838536	20.172453	70.980340
803.835438	21.311642	70.985345
802.847355	20.590722	70.990350
802.020495	14.238120	70.995354
801.198488	27.739987	71.000359
800.947236	22.193031	71.005364
800.824174	13.446563	71.010369
799.810362	22.686533	71.015374
798.964746	13.250848	71.020378
798.445136	18.659031	71.025383
797.875155	24.969361	71.030388
796.901267	13.934578	71.035393
796.112437	19.871316	71.040398
795.714599	14.505393	71.045402
794.542315	19.109160	71.050407
793.871597	19.818468	71.055412
793.663520	18.730534	71.060417
793.045690	30.804312	71.065422
792.888701	21.547581	71.070426
791.716044	19.334301	71.075431
790.737114	27.751870	71.080436
790.583832	14.736706	71.085441
789.763840	14.164073	71.090446
788.648095	15.395231	71.095450
788.104666	9.353905	71.100455
787.675505	16.247359	71.105460
787.538426	14.542579	71.110465
786.323183	20.671780	71.115470
785.398872	15.004896	71.120474
785.344878	22.172940	71.125479
784.717230	23.217590	71.130484
783.704525	19.833993	71.135489
782.698259	27.104750	71.140494
782.444133	16.691821	71.145498
782.353399	23.277516	71.150503
781.339187	19.113575	71.155508
780.817606	12.157301	71.160513
779.935639	14.092408	71.165518
778.448021	13.930410	71.170522
778.057385	19.366950	71.175527
777.272592	17.497205	71.180532
777.151787	17.729469	71.185537
776.571290	31.453092	71.190542
776.594137	17.388033	71.195546
775.470336	15.535988	71.200551
774.620515	24.447087	71.205556
773.565822	17.424296	71.210561
772.378287	20.701141	71.215566
772.094771	18.381015	71.220570
771.767036	20.634742	71.225575
771.173333	20.407709	71.230580
771.288603	22.064214	71.235585
770.184632	29.790496	71.240590
769.640695	21.541535	71.245594
768.537786	22.116229	71.250599
767.696384	27.607189	71.255604
767.151165	21.933575	71.260609
766.544019	22.328420	71.265614
766.258014	8.965393	71.270618
764.946606	24.495849	71.275623
764.202469	29.127663	71.280628
764.283981	17.029172	71.285633
763.536903	20.559172	71.290638
762.882815	14.227965	71.295642
762.022399	20.770614	71.300647
761.254844	16.409721	71.305652
760.969734	16.540412	71.310657
759.652501	23.669872	71.315662
759.297312	15.651063	71.320666
758.519619	16.785838	71.325671
757.962494	19.937094	71.330676
757.194587	14.909214	71.335681
755.985783	21.579869	71.340686
755.896562	23.426623	71.345690
755.409399	24.418952	71.350695
755.104854	18.170868	71.355700
754.342727	12.443485	71.360705
753.541836	18.487809	71.365710
752.965150	9.283718	71.370714
751.735094	14.841285	71.375719
750.830329	12.053948	71.380724
750.673360	14.586415	71.385729
750.485267	19.780979	71.390734
749.751046	13.214955	71.395738
748.599480	17.927405	71.400743
748.154985	17.960471	71.405748
747.961515	10.914123	71.410753
746.508683	14.195369	71.415758
746.127527	14.055927	71.420762
745.553740	15.957749	71.425767
744.866523	22.259943	71.430772
744.195306	11.738391	71.435777
743.452634	22.356030	71.440782
743.268532	9.159710	71.445786
742.153755	16.917678	71.450791
741.020100	8.183887	71.455796
740.773649	6.655795	71.460801
740.253489	23.738144	71.465806
739.539340	14.035551	71.470810
738.483620	11.455178	71.475815
738.142458	22.434667	71.480820
738.060640	12.464245	71.485825
736.411663	15.872919	71.490830
736.077561	12.455419	71.495834
735.539040	12.892961	71.500839
735.217987	11.952329	71.505844
734.256847	11.331225	71.510849
733.446604	17.512659	71.515854
733.041383	8.784319	71.520858
732.397106	16.235571	71.525863
731.385805	6.375295	71.530868
730.806437	15.591843	71.535873
730.094237	19.078452	71.540878
729.912823	14.813480	71.545882
728.797834	13.172941	71.550887
727.545970	12.558704	71.555892
727.454630	13.937443	71.560897
727.016498	21.117759	71.565902
726.654403	13.808104	71.570906
725.957328	16.653645	71.575911
724.959632	17.765111	71.580916
724.630324	8.980533	71.585921
723.471518	18.804998	71.590926
722.926110	10.600447	71.595930
722.297925	15.368345	71.600935
721.636438	16.844170	71.605940
721.350294	3.839147	71.610945
720.469835	17.050708	71.615950
719.836447	11.801153	71.620954
719.094807	14.259557	71.625959
717.851191	15.493759	71.630964
717.310137	14.320079	71.635969
716.613934	10.974428	71.640974
716.558913	10.469254	71.645978
716.033178	11.422000	71.650983
715.183301	3.062507	71.655988
714.601158	9.172932	71.660993
713.893213	14.989578	71.665998
713.459956	6.201055	71.671002
712.011902	20.100652	71.676007
711.313143	22.522270	71.681012
711.130966	16.363520	71.686017
710.680634	18.015460	71.691022
709.858439	15.951422	71.696026
708.756634	22.387443	71.701031
708.136268	22.202517	71.706036
708.053568	15.452346	71.711041
707.118072	25.692270	71.716046
706.326153	16.091957	71.721050
705.739563	12.935435	71.726055
705.389647	13.207337	71.731060
704.616089	7.928068	71.736065
703.407996	17.318845	71.741070
703.213017	18.837089	71.746074
702.919816	13.497103	71.751079
702.028444	17.475866	71.756084
701.242072	11.872212	71.761089
701.005153	26.283866	71.766094
699.822938	21.224203	71.771098
698.962602	15.275937	71.776103
698.197378	19.663543	71.781108
698.137403	13.084796	71.786113
697.388306	21.462639	71.791118
696.530519	14.145186	71.796122
695.853194	16.334739	71.801127
695.316584	21.532759	71.806132
694.923564	10.555350	71.811137
693.705783	13.753466	71.816142
693.337191	4.069991	71.821146
692.565893	10.297270	71.826151
691.528238	12.405428	71.831156
690.545914	17.171376	71.836161
690.190433	14.815412	71.841166
689.907427	13.838767	71.846170
689.542433	20.958555	71.851175
689.434173	13.419257	71.856180
688.327247	9.333202	71.861185
687.501816	19.792141	71.866190
686.893211	3.172095	71.871194
685.515551	15.232822	71.876199
684.988327	17.389014	71.881204
685.019122	10.417351	71.886209
684.146349	8.631033	71.891214
683.234657	5.289746	71.896218
682.641433	20.984985	71.901223
682.180251	21.924306	71.906228
681.569644	12.079094	71.911233
680.482995	20.605307	71.916238
680.151239	14.460918	71.921242
679.637137	16.534598	71.926247
678.361116	26.650559	71.931252
677.677240	15.432463	71.936257
676.960566	18.090328	71.941262
677.007109	9.491914	71.946266
676.560644	22.749497	71.951271
675.585779	21.318479	71.956276
675.090966	10.250052	71.961281
674.355807	19.936114	71.966286
673.345651	7.767049	71.971290
672.455630	13.699429	71.976295
671.944144	16.794549	71.981300
671.960523	8.191477	71.986305
670.874099	23.903756	71.991310
670.117566	10.423293	71.996314
669.424652	20.373861	72.001319
668.983299	13.571999	72.006324
668.251752	14.128601	72.011329
667.144770	19.037409	72.016334
666.752686	12.945208	72.021338
666.271099	18.943438	72.026343
665.812867	20.437374	72.031348
664.615775	8.742777	72.036353
664.049062	10.331256	72.041358
663.961825	8.027198	72.046362
663.121759	12.475614	72.051367
662.203876	15.023599	72.056372
661.643467	5.840604	72.061377
660.743461	10.960878	72.066382
659.949123	15.321590	72.071386
659.294809	17.507487	72.076391
658.833468	13.867413	72.081396
658.779305	15.804778	72.086401
657.753335	21.597966	72.091406
656.857546	9.253004	72.096410
656.202081	16.909475	72.101415
655.674628	22.057159	72.106420
655.082592	15.135793	72.111425
654.033703	21.115557	72.116430
653.702648	6.599111	72.121434
653.262580	15.219481	72.126439
652.065691	14.501911	72.131444
651.207347	14.643476	72.136449
650.490386	26.594283	72.141454
650.449162	21.280408	72.146458
650.013230	13.769642	72.151463
649.253324	17.929334	72.156468
649.014544	10.592176	72.161473
647.725649	17.185743	72.166478
646.766926	12.609333	72.171482
645.816452	22.714462	72.176487
645.630883	13.806085	72.181492
645.248406	15.481922	72.186497
644.486639	15.092452	72.191502
643.735369	16.093744	72.196506
642.910127	24.204608	72.201511
642.508322	19.364469	72.206516
641.980282	5.721480	72.211521
640.953855	14.870463	72.216526
640.173438	18.074647	72.221530
640.043226	9.280459	72.226535
639.172268	18.770535	72.231540
638.668063	12.257808	72.236545
637.626913	15.348974	72.241550
637.199936	14.092491	72.246554
636.414043	9.572141	72.251559
635.400838	17.276125	72.256564
635.050756	14.370537	72.261569
634.629225	18.459000	72.266574
634.125548	11.173492	72.271578
632.639429	9.314560	72.276583
632.239385	14.200684	72.281588
631.840087	6.844939	72.286593
631.339641	15.672044	72.291598
631.152203	8.389791	72.296602
630.288742	21.425204	72.301607
629.064072	17.419427	72.306612
628.253313	13.601621	72.311617
627.118181	22.141881	72.316622
627.150113	14.665419	72.321626
626.832959	17.470980	72.326631
626.473305	14.284647	72.331636
625.333947	8.257849	72.336641
624.489088	19.096783	72.341646
624.361673	8.558061	72.346650
623.203732	12.192952	72.351655
622.234464	7.807465	72.356660
621.880826	5.402336	72.361665
621.170599	11.086903	72.366670
620.600750	4.119442	72.371674
619.655130	2.209133	72.376679
619.121482	7.080264	72.381684
618.839112	2.897619	72.386689
618.352395	5.812184	72.391694
617.581735	5.543986	72.396698
616.669205	5.389844	72.401703
616.322002	11.778256	72.406708
615.222055	5.437686	72.411713
614.282509	7.963905	72.416718
613.992392	9.360112	72.421722
613.525794	5.277769	72.426727
612.683500	9.871632	72.431732
612.032419	9.975470	72.436737
611.352068	19.859393	72.441742
611.034720	10.667662	72.446746
609.868465	17.194406	72.451751
609.113123	11.076494	72.456756
608.932806	9.104228	72.461761
608.053637	18.991430	72.466766
606.942588	9.818877	72.471770
606.270905	12.781828	72.476775
605.983498	8.863333	72.481780
605.804780	13.118128	72.486785
605.211291	19.845387	72.491790
604.195841	12.783317	72.496794
603.630235	11.843806	72.501799
602.683661	17.733177	72.506804
601.940927	14.795514	72.511809
601.038694	17.719493	72.516814
600.856979	19.117360	72.521818
600.345911	13.345318	72.526823
599.710688	15.438303	72.531828
598.872922	9.598449	72.536833
597.876213	21.128618	72.541838
597.743314	16.471163	72.546842
596.616429	10.434508	72.551847
595.761555	9.556840	72.556852
595.184480	5.060017	72.561857
594.968115	14.524692	72.566862
594.755759	4.336971	72.571866
593.590179	10.054643	72.576871
592.907603	19.746537	72.581876
592.651877	11.079577	72.586881
591.148499	16.311742	72.591886
590.582474	1.276085	72.596890
589.934100	2.377698	72.601895
589.580045	6.907996	72.606900
589.555201	6.435865	72.611905
588.390677	9.387429	72.616910
587.496620	7.467343	72.621914
586.748249	25.543244	72.626919
586.325262	20.955645	72.631924
585.540303	15.471655	72.636929
584.877710	18.401625	72.641934
584.625749	21.337155	72.646938
583.505985	10.849262	72.651943
582.499341	19.086800	72.656948
582.369765	20.528403	72.661953
581.678865	23.167996	72.666958
581.588420	13.463896	72.671962
580.326133	17.747777	72.676967
579.508509	14.902474	72.681972
579.025216	12.844427	72.686977
577.740878	22.184322	72.691982
577.208092	17.358751	72.696986
577.020875	11.093593	72.701991
576.609097	19.195386	72.706996
576.258908	10.513513	72.712001
575.192041	22.438059	72.717006
574.502569	11.859557	72.722010
573.746809	14.083709	72.727015
572.905897	21.895890	72.732020
572.502996	10.393393	72.737025
571.594269	17.282828	72.742030
571.169260	15.832081	72.747034
570.308021	18.672271	72.752039
569.535201	22.092882	72.757044
569.542155	14.180438	72.762049
568.573136	26.049980	72.767054
567.401747	18.694223	72.772058
567.240496	15.074180	72.777063
566.334524	20.312129	72.782068
566.083296	6.142535	72.787073
565.321432	18.920506	72.792078
564.464366	24.133321	72.797082
563.859481	27.418378	72.802087
563.005436	20.663350	72.807092
562.318791	21.942952	72.812097
561.263803	22.207332	72.817102
561.281273	18.109395	72.822106
560.589302	25.003736	72.827111
559.979286	20.043815	72.832116
559.438962	18.106818	72.837121
558.591942	27.903763	72.842126
558.329859	21.563797	72.847130
557.037239	20.300133	72.852135
555.959439	24.337024	72.857140
555.735151	16.278489	72.862145
555.318198	24.912537	72.867150
554.880457	18.146395	72.872154
554.041051	17.684165	72.877159
553.104914	24.330396	72.882164
553.103279	17.089518	72.887169
551.502719	20.902175	72.892174
551.271453	19.726496	72.897178
550.621466	17.389082	72.902183
549.939248	23.163823	72.907188
549.270855	16.634694	72.912193
548.272551	26.198698	72.917198
547.946888	16.259258	72.922202
547.388477	24.521605	72.927207
546.809772	21.578333	72.932212
546.113820	16.103833	72.937217
545.175608	16.103617	72.942222
545.043154	18.258454	72.947226
543.642861	21.132479	72.952231
542.687052	26.840418	72.957236
542.717516	14.160310	72.962241
541.880185	21.774812	72.967246
541.836521	23.917083	72.972250
540.606796	17.685527	72.977255
540.061688	16.944613	72.982260
539.602938	16.171020	72.987265
538.591975	21.575511	72.992270
537.785501	19.497991	72.997274
537.384685	19.807985	73.002279
537.064307	27.816379	73.007284
536.264564	14.320779	73.012289
535.332541	19.854620	73.017294
534.703091	16.134122	73.022298
534.464895	18.097647	73.027303
533.560498	23.750091	73.032308
533.179207	17.941623	73.037313
532.122463	23.681412	73.042318
531.185770	11.656836	73.047322
530.160094	19.705037	73.052327
529.743627	21.551883	73.057332
529.909342	21.118783	73.062337
528.936917	25.004859	73.067342
527.993305	14.859514	73.072346
527.665730	12.828712	73.077351
526.819688	11.574351	73.082356
526.499297	19.639512	73.087361
525.318312	17.509692	73.092366
524.885568	16.894384	73.097370
524.372878	17.723667	73.102375
523.312076	27.248749	73.107380
522.743790	19.779597	73.112385
521.912986	27.564953	73.117390
521.507035	15.984105	73.122394
521.163844	20.364451	73.127399
520.243604	19.309566	73.132404
519.836128	14.984439	73.137409
519.027753	23.360724	73.142414
518.131770	12.718948	73.147418
517.560159	21.428096	73.152423
516.820734	17.892276	73.157428
516.684454	17.248665	73.162433
515.110169	12.753026	73.167438
514.505584	7.282909	73.172442
514.075933	16.839907	73.177447
513.844595	17.105561	73.182452
513.533332	7.685807	73.187457
512.524641	16.112924	73.192462
511.992111	22.398408	73.197466
510.796862	19.865595	73.202471
509.700107	22.338050	73.207476
509.706710	17.424995	73.212481
509.063170	22.897120	73.217486
508.421401	14.586559	73.222490
507.694524	21.726163	73.227495
506.669216	23.319925	73.232500
506.234714	18.057675	73.237505
505.537723	25.582023	73.242510
505.122995	18.741265	73.247514
504.497446	22.895362	73.252519
503.649326	21.308606	73.257524
503.067540	15.916858	73.262529
502.316148	25.700157	73.267534
501.734726	16.064821	73.272538
501.242023	21.287416	73.277543
500.239751	13.959950	73.282548
499.907806	13.719668	73.287553
498.892531	19.940134	73.292558
498.500621	13.100476	73.297562
497.684152	19.130000	73.302567
497.059526	21.938827	73.307572
496.357566	14.856829	73.312577
495.286285	25.788637	73.317582
495.152476	18.967783	73.322586
494.770193	19.763681	73.327591
493.697802	18.827662	73.332596
493.231357	11.449531	73.337601
492.981580	18.735477	73.342606
492.052911	19.642075	73.347610
491.226440	19.914233	73.352615
490.518324	23.441252	73.357620
489.943550	19.847671	73.362625
489.003522	24.428759	73.367630
488.348107	18.436894	73.372634
487.958852	19.957717	73.377639
487.538363	25.629276	73.382644
486.545949	13.389673	73.387649
485.726529	17.831698	73.392654
485.565934	19.538441	73.397658
484.590216	23.964368	73.402663
483.300263	22.203585	73.407668
482.939365	14.086404	73.412673
482.235594	16.029490	73.417678
482.321286	17.104068	73.422682
481.126198	17.195262	73.427687
480.455914	21.455838	73.432692
480.241085	15.299169	73.437697
479.488702	21.842031	73.442702
478.721483	12.633693	73.447706
478.003835	17.133622	73.452711
477.387683	19.575254	73.457716
476.501821	17.461518	73.462721
475.310206	17.303006	73.467726
475.068084	13.039853	73.472730
474.848767	17.397314	73.477735
474.174003	11.224038	73.482740
473.290866	14.881443	73.487745
472.456121	17.996560	73.492750
472.160118	15.206962	73.497754
471.610069	13.741462	73.502759
470.518520	17.444688	73.507764
469.916564	11.997819	73.512769
469.451170	19.188809	73.517774
469.211091	13.080320	73.522778
467.934437	12.361357	73.527783
466.988757	10.936813	73.532788
467.041162	6.929510	73.537793
465.968349	15.601820	73.542798
465.348440	17.652974	73.547802
464.684389	13.822893	73.552807
464.066826	18.496112	73.557812
463.720681	12.771948	73.562817
462.529026	20.247381	73.567822
461.782172	13.629860	73.572826
461.225330	17.588517	73.577831
460.733237	17.178216	73.582836
460.708324	14.381698	73.587841
459.551070	20.340950	73.592846
458.755541	13.500953	73.597850
458.021272	18.680040	73.602855
457.039032	28.358206	73.607860
456.841784	20.285916	73.612865
455.840137	24.850025	73.617870
455.778980	11.607370	73.622874
455.238530	17.898853	73.627879
454.208122	16.727507	73.632884
453.825851	15.216357	73.637889
452.712521	21.308961	73.642894
451.825494	15.040202	73.647898
451.523175	14.490858	73.652903
450.962934	19.962337	73.657908
450.351427	16.789354	73.662913
448.996028	24.663039	73.667918
449.132754	11.275319	73.672922
448.689692	18.035404	73.677927
447.054247	21.093602	73.682932
446.818164	15.157941	73.687937
445.681370	27.293941	73.692942
445.506438	29.830861	73.697946
445.365400	21.708617	73.702951
444.368756	31.154120	73.707956
443.777310	13.660965	73.712961
442.755464	25.546841	73.717966
442.566364	19.961657	73.722970
441.514681	19.110670	73.727975
440.621973	19.096935	73.732980
440.538384	12.725400	73.737985
439.825063	22.076872	73.742990
438.686349	15.014022	73.747994
438.186404	19.228543	73.752999
437.464954	18.719174	73.758004
437.556381	11.059785	73.763009
436.323185	16.472911	73.768014
435.834472	18.479513	73.773018
435.325708	16.341979	73.778023
434.001688	15.127538	73.783028
433.585480	12.101637	73.788033
432.721862	24.812270	73.793038
432.831723	13.880961	73.798042
431.619144	17.715449	73.803047
430.692834	11.992270	73.808052
430.261169	18.838850	73.813057
429.499545	29.943690	73.818062
429.340611	16.904269	73.823066
428.653832	16.955497	73.828071
427.557701	21.965172	73.833076
427.616804	7.787166	73.838081
426.110798	21.027502	73.843086
425.201046	18.635320	73.848090
424.550851	24.937990	73.853095
424.472171	32.105220	73.858100
424.190898	23.188471	73.863105
423.379977	23.961216	73.868110
422.728354	23.811304	73.873114
422.167840	21.248361	73.878119
420.840913	23.402719	73.883124
420.165974	19.143883	73.888129
419.541352	22.493614	73.893134
419.237116	17.560707	73.898138
419.071830	20.331052	73.903143
417.786111	21.742418	73.908148
417.644621	14.351951	73.913153
416.577924	18.052816	73.918158
415.600996	11.509820	73.923162
414.653115	11.515925	73.928167
414.382249	16.454028	73.933172
414.074372	8.426188	73.938177
413.366286	16.221972	73.943182
412.681522	13.346098	73.948186
412.108399	21.320651	73.953191
411.360012	16.223555	73.958196
410.410038	5.885326	73.963201
409.448041	15.006768	73.968206
409.248444	8.138067	73.973210
408.838856	7.528552	73.978215
408.143631	20.537202	73.983220
407.512971	14.626575	73.988225
407.102664	12.648398	73.993230
406.111986	11.016586	73.998234
405.540414	6.823288	74.003239
404.579324	15.856280	74.008244
403.984704	9.608758	74.013249
402.727226	20.228065	74.018254
402.145345	15.648483	74.023258
401.906939	20.753301	74.028263
401.298442	13.358405	74.033268
401.020579	16.610307	74.038273
399.933546	18.038907	74.043278
399.371518	15.450981	74.048282
399.091663	19.259857	74.053287
397.922658	17.940312	74.058292
397.407334	18.565039	74.063297
396.635324	21.031525	74.068302
396.162343	25.307988	74.073306
395.339833	15.545528	74.078311
394.388599	19.617506	74.083316
393.812016	11.996758	74.088321
393.570719	22.736413	74.093326
392.944965	16.894394	74.098330
391.969339	14.806033	74.103335
391.308844	16.002666	74.108340
391.076670	14.158530	74.113345
390.059514	13.380910	74.118350
389.307416	19.024895	74.123354
388.437452	9.732046	74.128359
388.034435	21.449937	74.133364
388.002030	12.772662	74.138369
386.710351	19.969177	74.143374
386.260437	16.466114	74.148378
385.387283	18.199678	74.153383
384.943006	22.187720	74.158388
383.959421	12.525051	74.163393
383.361073	14.530210	74.168398
382.966855	5.544748	74.173402
381.969648	14.077306	74.178407
380.832662	16.240839	74.183412
380.517891	17.546383	74.188417
379.961381	20.278149	74.193422
380.043148	18.573218	74.198426
379.496417	13.887117	74.203431
378.352218	19.615666	74.208436
377.897258	2.848269	74.213441
376.688074	8.454708	74.218446
376.016572	3.025261	74.223450
375.518833	14.111700	74.228455
375.049375	8.232167	74.233460
374.382687	14.009198	74.238465
373.474312	14.996182	74.243470
372.620586	12.069977	74.248474
372.588204	13.223289	74.253479
371.417000	21.750467	74.258484
370.672628	15.846934	74.263489
369.959786	22.568021	74.268494
369.957639	11.189374	74.273498
369.435994	15.391592	74.278503
368.182624	5.488082	74.283508
367.920221	13.764775	74.288513
366.982766	19.439882	74.293518
366.048994	15.846777	74.298522
365.686310	19.549009	74.303527
365.187351	22.681610	74.308532
364.883184	12.905946	74.313537
363.223110	15.394117	74.318542
363.038023	10.065349	74.323546
362.414892	12.790388	74.328551
362.026186	14.033601	74.333556
360.826165	4.742904	74.338561
360.310253	10.172637	74.343566
359.818781	8.152212	74.348570
359.248611	9.529998	74.353575
357.871733	13.139970	74.358580
357.609231	9.274316	74.363585
357.069231	16.713746	74.368590
356.561783	15.503255	74.373594
355.578970	16.081068	74.378599
354.568248	12.126499	74.383604
354.536905	9.247435	74.388609
354.255477	21.743877	74.393614
353.445895	10.039754	74.398618
352.554381	16.503892	74.403623
351.715277	21.202980	74.408628
351.094989	16.003491	74.413633
350.060629	13.412005	74.418638
349.591199	13.789734	74.423642
349.359738	4.814612	74.428647
348.673724	14.190128	74.433652
347.936648	10.978841	74.438657
346.897862	20.060503	74.443662
346.679827	15.396143	74.448666
346.031692	12.992262	74.453671
344.658991	9.248350	74.458676
344.517725	6.568152	74.463681
344.140205	14.355421	74.468686
343.312080	18.519757	74.473690
342.201090	16.295297	74.478695
341.646194	26.682816	74.483700
341.271180	9.737105	74.488705
340.669196	17.542803	74.493710
339.952181	20.970353	74.498714
339.289435	17.343527	74.503719
338.344704	14.630531	74.508724
338.407966	10.120036	74.513729
336.932508	24.181858	74.518734
336.194314	12.906327	74.523738
335.839380	16.080632	74.528743
335.116848	13.120916	74.533748
335.298562	5.335184	74.538753
334.081786	23.028449	74.543758
333.119978	27.764445	74.548762
332.652736	12.594866	74.553767
331.733938	21.179601	74.558772
331.194022	18.791592	74.563777
330.545024	25.202897	74.568782
330.329574	20.359932	74.573786
329.589753	16.535661	74.578791
328.493336	18.278019	74.583796
328.218545	15.871410	74.588801
327.492018	20.260830	74.593806
326.582816	19.286261	74.598810
325.919344	19.324342	74.603815
325.352812	14.177794	74.608820
325.088698	21.477069	74.613825
324.042473	26.079868	74.618830
323.530497	14.672094	74.623834
323.092623	19.125894	74.628839
322.083401	18.201961	74.633844
321.382793	14.171173	74.638849
320.632614	10.099403	74.643854
320.104092	12.692680	74.648858
319.185843	13.182947	74.653863
318.162820	13.502259	74.658868
318.510304	14.470451	74.663873
317.622779	15.242823	74.668878
316.698317	14.084613	74.673882
315.759062	9.478438	74.678887
315.177656	24.470088	74.683892
315.265060	8.004190	74.688897
314.312244	9.176471	74.693902
313.465559	19.566340	74.698906
313.062139	13.753565	74.703911
312.284134	17.417920	74.708916
311.358391	13.329980	74.713921
310.338441	22.635731	74.718926
310.268583	9.142182	74.723930
309.972980	13.686846	74.728935
308.540486	12.403033	74.733940
308.045149	6.674298	74.738945
307.083141	11.996948	74.743950
307.148471	6.795430	74.748954
306.411134	11.722731	74.753959
305.686196	17.578447	74.758964
305.153297	-0.207810	74.763969
304.167330	14.346848	74.768974
303.372813	13.544818	74.773978
302.796065	8.008829	74.778983
302.293844	20.133612	74.783988
302.016840	10.076096	74.788993
300.608653	13.976512	74.793998
299.890933	10.175538	74.799002
299.424675	23.261250	74.804007
299.127812	18.664652	74.809012
298.703662	7.372202	74.814017
297.559619	20.070787	74.819022
296.976928	16.186790	74.824026
296.610910	6.749006	74.829031
295.307907	11.499970	74.834036
294.734087	5.275977	74.839041
294.082088	11.575799	74.844046
293.832306	5.874160	74.849050
293.314476	13.369987	74.854055
292.052107	12.032260	74.859060
291.863075	2.979426	74.864065
290.890650	16.871198	74.869070
290.347691	15.650612	74.874074
289.209898	15.292804	74.879079
288.338069	7.359612	74.884084
288.207960	3.881292	74.889089
287.981707	13.047920	74.894094
287.708798	9.149243	74.899098
286.427269	11.056739	74.904103
285.706517	15.661287	74.909108
285.389430	9.730682	74.914113
284.023326	16.647373	74.919118
283.524040	4.725095	74.924122
283.210546	9.368804	74.929127
282.684725	15.486095	74.934132
281.895402	11.934656	74.939137
281.152867	12.631892	74.944142
280.596757	1.838295	74.949146
279.531105	15.467389	74.954151
278.558070	19.333149	74.959156
278.415087	14.437642	74.964161
277.743125	21.546465	74.969166
277.669196	10.554581	74.974170
276.767590	15.831345	74.979175
275.715336	23.986368	74.984180
275.553076	10.122782	74.989185
274.189878	16.482359	74.994190
273.567757	7.222596	74.999194
273.059115	10.768332	75.004199
272.568687	8.888106	75.009204
272.229651	9.166218	75.014209
271.180950	10.760647	75.019214
270.419179	11.136105	75.024218
270.310898	15.253527	75.029223
268.939216	13.613120	75.034228
268.403321	10.447061	75.039233
267.724416	10.908657	75.044238
267.299551	15.633199	75.049242
266.996114	11.255273	75.054247
265.905565	25.825045	75.059252
265.534516	8.131265	75.064257
264.535162	12.622534	75.069262
263.586028	13.693324	75.074266
263.111956	12.945882	75.079271
262.293772	18.818048	75.084276
261.955849	13.756502	75.089281
261.694585	13.230600	75.094286
260.984050	13.640471	75.099290
260.115910	10.252989	75.104295
259.295426	22.100508	75.109300
258.522299	13.924515	75.114305
257.675500	13.938221	75.119310
257.440533	16.681833	75.124314
256.939991	15.437148	75.129319
255.523810	12.468183	75.134324
255.084472	13.320519	75.139329
254.129199	11.479704	75.144334
253.792243	13.604070	75.149338
253.698479	8.060490	75.154343
252.992926	9.608111	75.159348
252.538019	15.591102	75.164353
251.730904	17.104452	75.169358
250.764029	18.102382	75.174362
250.108027	18.478332	75.179367
249.173849	22.904027	75.184372
248.880818	12.674037	75.189377
247.829714	18.187528	75.194382
246.806517	13.444955	75.199386
246.488237	7.002047	75.204391
245.761248	17.691389	75.209396
245.820524	15.463347	75.214401
245.245394	18.939264	75.219406
244.392830	15.501996	75.224410
243.895691	6.712746	75.229415
242.717593	16.310226	75.234420
241.959131	9.456525	75.239425
241.136984	21.531390	75.244430
240.659537	10.012489	75.249434
240.393628	9.200329	75.254439
239.796892	15.898202	75.259444
239.511619	9.951496	75.264449
238.174378	18.174036	75.269454
237.373332	13.086976	75.274458
236.679641	10.337157	75.279463
236.252496	11.277438	75.284468
235.844141	10.838064	75.289473
234.485578	16.947767	75.294478
234.226017	20.081649	75.299482
233.691744	22.057704	75.304487
232.635469	13.426973	75.309492
232.342868	11.220334	75.314497
231.415796	16.147940	75.319502
231.088876	13.003768	75.324506
230.570486	16.789182	75.329511
229.408213	23.518870	75.334516
228.817422	11.432999	75.339521
228.288025	17.136137	75.344526
228.003000	21.933008	75.349530
227.011388	13.889627	75.354535
225.978034	21.089188	75.359540
225.753108	18.553220	75.364545
225.213935	14.463613	75.369550
224.078856	16.994335	75.374554
223.193817	22.342593	75.379559
223.087496	18.622367	75.384564
222.791143	12.284774	75.389569
221.398474	24.720253	75.394574
220.580028	10.450362	75.399578
220.553225	11.823555	75.404583
220.222374	18.368660	75.409588
219.027730	10.266191	75.414593
217.962381	22.947527	75.419598
217.604350	15.285685	75.424602
217.287918	12.305421	75.429607
216.240305	19.064140	75.434612
215.813128	11.534747	75.439617
214.746365	22.705613	75.444622
214.618927	15.290856	75.449626
213.632974	16.060034	75.454631
212.602730	19.934938	75.459636
212.469030	17.087966	75.464641
211.806383	20.432765	75.469646
211.563703	12.828228	75.474650
210.645306	12.217864	75.479655
209.688943	17.438725	75.484660
209.360884	6.252406	75.489665
208.211057	14.101309	75.494670
207.427929	12.915879	75.499674
207.303081	10.206267	75.504679
206.597170	16.361742	75.509684
205.727567	2.191484	75.514689
204.906367	13.167081	75.519694
204.547273	10.863816	75.524698
204.429662	14.426069	75.529703
202.828874	16.285160	75.534708
202.838296	13.246641	75.539713
201.740521	21.093559	75.544718
201.020255	20.733880	75.549722
200.162743	12.916712	75.554727
199.531988	17.270393	75.559732
199.122465	15.079245	75.564737
198.857279	23.146659	75.569742
198.355105	16.092841	75.574746
197.218144	14.438708	75.579751
196.587257	19.013182	75.584756
196.201450	14.137475	75.589761
195.120409	22.560461	75.594766
194.549935	14.390031	75.599770
194.020265	14.559777	75.604775
193.179340	17.374771	75.609780
192.467282	8.340684	75.614785
191.778674	15.477405	75.619790
191.196227	15.624028	75.624794
191.004858	15.260452	75.629799
189.809912	22.785405	75.634804
189.178391	14.834441	75.639809
188.751959	13.696225	75.644814
187.926835	12.314072	75.649818
186.892944	13.401558	75.654823
186.219183	17.779446	75.659828
186.404028	14.798112	75.664833
185.891913	22.879664	75.669838
185.033542	16.513412	75.674842
184.088535	15.885223	75.679847
183.239429	17.652867	75.684852
182.618331	12.418868	75.689857
181.365650	17.691713	75.694862
180.980886	19.918327	75.699866
180.674364	15.594523	75.704871
180.109562	14.926217	75.709876
180.049088	10.716147	75.714881
178.736130	19.972461	75.719886
177.976608	15.284074	75.724890
177.945351	13.575083	75.729895
176.579372	25.664133	75.734900
175.834350	12.562099	75.739905
175.571874	17.823725	75.744910
175.032757	10.268036	75.749914
174.179896	11.659396	75.754919
173.419430	5.979276	75.759924
172.936086	7.464682	75.764929
171.553901	20.803663	75.769934
171.188698	15.587213	75.774938
170.887274	13.419836	75.779943
170.119533	18.790406	75.784948
170.112387	15.010219	75.789953
168.825888	17.554070	75.794958
168.147672	16.514348	75.799962
167.777427	15.259946	75.804967
166.416870	16.831603	75.809972
166.051668	20.248834	75.814977
165.352411	24.037868	75.819982
165.073141	17.858407	75.824986
164.735309	14.268138	75.829991
163.489478	21.723945	75.834996
163.140088	14.732509	75.840001
162.482686	17.887252	75.845006
161.098805	13.041382	75.850010
160.490715	10.407247	75.855015
159.843239	14.539679	75.860020
159.887514	9.142829	75.865025
159.238559	9.367871	75.870030
158.333216	5.525900	75.875034
157.572671	8.719165	75.880039
157.021658	14.378451	75.885044
156.401417	11.725754	75.890049
155.720554	9.871188	75.895054
155.202744	7.071275	75.900058
154.308390	-3.534303	75.905063
153.102739	17.019354	75.910068
152.964962	4.446554	75.915073
152.391286	14.941157	75.920078
152.028412	13.660352	75.925082
151.057143	5.191153	75.930087
150.075021	8.257327	75.935092
149.645897	12.619868	75.940097
148.956579	16.246473	75.945102
148.309662	9.773984	75.950106
147.531193	2.067242	75.955111
147.058044	4.243297	75.960116
146.947392	12.103142	75.965121
145.763506	15.775491	75.970126
144.743888	15.422561	75.975130
144.517635	7.725534	75.980135
143.547977	14.126500	75.985140
142.625522	8.076412	75.990145
142.111201	13.603695	75.995150
141.644746	11.817445	76.000154
141.208615	10.843208	76.005159
140.524785	19.756377	76.010164
140.007197	10.558838	76.015169
139.394431	9.005650	76.020174
138.842824	4.605820	76.025178
138.058122	1.506277	76.030183
137.123438	10.353786	76.035188
136.704855	7.419786	76.040193
135.339641	17.763068	76.045198
134.556498	1.260979	76.050202
134.133691	12.122603	76.055207
133.479185	12.337499	76.060212
133.426416	7.560088	76.065217
132.845719	15.286731	76.070222
131.861826	5.245782	76.075226
131.469057	6.286252	76.080231
130.678682	8.159662	76.085236
129.594704	7.077423	76.090241
128.794165	-0.237867	76.095246
128.499866	-1.982180	76.100250
127.912898	0.516374	76.105255
127.463234	10.273701	76.110260
126.613639	5.951352	76.115265
125.933436	7.021887	76.120270
125.013992	10.128537	76.125274
124.673535	9.443394	76.130279
123.495341	9.713415	76.135284
123.360691	7.215104	76.140289
122.566254	7.934856	76.145294
122.091960	4.599743	76.150298
121.322919	7.449025	76.155303
120.422634	6.179806	76.160308
120.329892	-4.454234	76.165313
119.419761	7.975290	76.170318
118.441336	7.024455	76.175322
118.039402	6.019539	76.180327
117.505100	8.750968	76.185332
116.589446	1.283730	76.190337
115.399974	3.990325	76.195342
115.162267	-3.493555	76.200346
115.005902	4.780421	76.205351
114.189580	10.442596	76.210356
113.300558	-1.668202	76.215361
112.656385	12.570227	76.220366
112.276348	1.786458	76.225370
111.444291	6.713141	76.230375
110.732032	10.958413	76.235380
110.373176	2.533501	76.240385
109.387358	0.585656	76.245390
108.427054	6.732831	76.250394
107.762087	5.771438	76.255399
107.492035	4.262954	76.260404
107.145840	-1.191469	76.265409
105.786711	0.392607	76.270414
105.524298	-5.303829	76.275418
104.687977	1.227266	76.280423
104.098972	5.743037	76.285428
103.353901	4.411227	76.290433
102.298041	10.267720	76.295438
102.137875	8.331712	76.300442
101.903861	5.128594	76.305447
100.554783	8.784728	76.310452
100.204733	-1.869779	76.315457
99.279915	12.110636	76.320462
99.098609	-2.066824	76.325466
98.433747	0.573465	76.330471
97.177538	11.167454	76.335476
97.124050	7.503470	76.340481
96.179491	5.919628	76.345486
95.440931	0.940931	76.350490
94.714752	-3.110929	76.355495
94.202289	7.261952	76.360500
93.978592	-1.712777	76.365505
92.644332	7.901772	76.370510
92.315952	7.493824	76.375514
91.818548	1.211977	76.380519
90.539025	16.478965	76.385524
89.925316	4.403115	76.390529
88.906691	8.120095	76.395534
88.677469	-2.309254	76.400538
88.660743	4.745566	76.405543
87.452556	4.213002	76.410548
86.949372	-1.891305	76.415553
86.229864	8.617096	76.420558
85.952161	5.241178	76.425562
84.979119	2.660536	76.430567
84.188488	6.571388	76.435572
83.669439	4.847154	76.440577
83.055511	6.681402	76.445582
82.324038	7.064701	76.450586
81.607206	4.947817	76.455591
80.638802	6.456980	76.460596
80.528109	9.540321	76.465601
79.857867	11.864513	76.470606
78.874878	3.517067	76.475610
78.413757	9.977299	76.480615
77.713103	16.584541	76.485620
77.151227	2.313236	76.490625
76.074463	6.954108	76.495630
75.636622	10.130623	76.500634
75.009195	4.189631	76.505639
74.468317	13.458472	76.510644
73.630331	4.364094	76.515649
73.094917	15.201105	76.520654
72.645448	5.265765	76.525658
72.070466	13.344735	76.530663
70.791935	18.787331	76.535668
70.805246	9.847339	76.540673
70.033126	11.665819	76.545678
69.222986	10.839551	76.550682
68.465173	4.520394	76.555687
67.495050	12.469998	76.560692
66.720238	9.786786	76.565697
66.099867	4.287788	76.570702
65.442257	2.339656	76.575706
65.322477	3.226214	76.580711
64.877093	11.735517	76.585716
64.527092	7.301977	76.590721
63.254786	8.342383	76.595726
62.609326	11.370666	76.600730
61.951724	10.666727	76.605735
60.969142	6.824499	76.610740
60.798679	5.812638	76.615745
59.552225	14.463894	76.620750
58.881621	8.890908	76.625754
58.450372	4.624866	76.630759
57.814823	4.967643	76.635764
57.683623	-2.654636	76.640769
56.529780	8.351964	76.645774
55.742256	6.583823	76.650778
55.262260	3.648597	76.655783
54.007765	8.578017	76.660788
53.358731	8.481407	76.665793
53.296654	9.253109	76.670798
52.788277	3.838753	76.675802
52.569328	-1.153414	76.680807
51.297078	8.585303	76.685812
50.742700	6.486672	76.690817
50.049155	9.921588	76.695822
49.144023	4.439627	76.700826
48.512942	9.146621	76.705831
47.674849	13.990710	76.710836
47.452491	-7.954424	76.715841
46.915996	-0.239557	76.720846
45.877918	0.258885	76.725850
45.501712	11.016888	76.730855
44.546825	10.888638	76.735860
44.012131	1.140363	76.740865
43.250881	11.314816	76.745870
42.433584	11.748085	76.750874
42.153387	2.455951	76.755879
41.204617	1.703842	76.760884
40.645632	7.880070	76.765889
40.001337	17.916028	76.770894
39.489348	8.217745	76.775898
39.103459	5.398397	76.780903
37.438275	7.050247	76.785908
37.165525	1.245085	76.790913
36.679665	17.131392	76.795918
36.328474	7.238733	76.800922
35.546023	-4.490059	76.805927
34.425400	4.421825	76.810932
34.184672	-3.176675	76.815937
33.641442	9.907121	76.820942
32.737624	11.212040	76.825946
32.182714	-1.026122	76.830951
31.383653	6.303283	76.835956
31.016792	7.882097	76.840961
30.016446	1.801908	76.845966
29.465655	3.011098	76.850970
28.941225	-1.296842	76.855975
27.968752	9.422225	76.860980
27.463657	4.101968	76.865985
26.510151	8.228046	76.870990
26.364396	7.956556	76.875994
25.927233	-1.938152	76.880999
24.515215	9.751447	76.886004
24.392198	-1.612598	76.891009
23.703021	7.708284	76.896014
22.794187	6.882004	76.901018
22.005824	0.545662	76.906023
21.642597	5.263553	76.911028
21.313692	4.688544	76.916033
19.879813	10.241092	76.921038
19.134182	1.876318	76.926042
18.659157	5.134464	76.931047
18.162022	13.622064	76.936052
17.941296	4.035026	76.941057
16.564626	10.234451	76.946062
15.995448	3.741726	76.951066
15.857996	-4.176012	76.956071
15.078993	8.559045	76.961076
14.275239	2.258275	76.966081
13.246393	6.366413	76.971086
13.010134	3.119512	76.976090
12.783926	-0.605222	76.981095
11.594830	5.408169	76.986100
10.904015	3.790196	76.991105
10.370099	0.447274	76.996110
9.739769	1.839462	77.001114
8.935412	-3.497707	77.006119
8.299012	13.246801	77.011124
8.242038	5.089145	77.016129
6.653011	5.022637	77.021134
5.911487	-0.844938	77.026139
5.599402	1.425296	77.031143
4.865474	4.951818	77.036148
4.664878	-3.141924	77.041153
3.718924	-2.834774	77.046158