Mon Mar 08 17:57:15 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.202348	103.263456	0.000000
-0.117193	86.452514	0.005005
-0.922453	52.234135	0.010010
-3.031886	8.090585	0.015014
-7.189777	2.856315	0.020019
-12.602069	12.154753	0.025024
-16.900798	3.273476	0.030029
-21.591823	12.707611	0.035034
-25.772738	17.444745	0.040038
-29.237338	8.465122	0.045043
-32.841521	9.615816	0.050048
-36.657419	14.714200	0.055053
-40.442253	18.371063	0.060058
-43.893492	21.676677	0.065062
-47.443502	6.467687	0.070067
-51.796410	18.754200	0.075072
-54.925922	12.911263	0.080077
-58.945245	1.675309	0.085082
-62.846498	20.553839	0.090086
-66.376192	8.508089	0.095091
-70.549801	17.848732	0.100096
-74.109330	12.017656	0.105101
-77.562681	12.496239	0.110106
-82.106748	19.937474	0.115110
-85.545506	14.591760	0.120115
-89.288657	18.636276	0.125120
-92.611854	17.783697	0.130125
-96.627940	8.310282	0.135130
-100.674777	10.004776	0.140134
-104.398728	10.173343	0.145139
-107.823710	17.997453	0.150144
-111.303571	7.189590	0.155149
-115.277944	12.742299	0.160154
-118.882754	2.465309	0.165158
-122.845868	-6.237505	0.170163
-127.071079	11.574762	0.175168
-131.088496	3.266964	0.180173
-134.532101	1.080664	0.185178
-138.465159	6.484893	0.190182
-142.103131	-0.451589	0.195187
-146.271841	8.803236	0.200192
-149.728238	16.783798	0.205197
-153.548443	7.785418	0.210202
-157.224283	12.218253	0.215206
-160.493255	4.243651	0.220211
-164.486131	18.000929	0.225216
-167.824159	13.060301	0.230221
-172.081671	14.507841	0.235226
-176.029162	9.128332	0.240230
-179.551235	7.356732	0.245235
-183.445251	8.430901	0.250240
-186.911989	10.253732	0.255245
-190.529002	9.195872	0.260250
-194.376993	13.433890	0.265254
-198.015895	11.496462	0.270259
-202.262939	12.073504	0.275264
-205.818710	12.125502	0.280269
-209.624282	6.762825	0.285274
-213.584280	23.285574	0.290278
-217.265598	15.268049	0.295283
-220.817364	20.912749	0.300288
-224.483751	13.892618	0.305293
-227.932402	26.768376	0.310298
-232.342367	24.184526	0.315302
-235.719153	15.587006	0.320307
-239.895692	17.923737	0.325312
-243.548607	18.294063	0.330317
-247.254367	4.436448	0.335322
-251.175631	16.745858	0.340326
-254.846450	12.833006	0.345331
-258.625739	16.429393	0.350336
-262.418273	13.278707	0.355341
-266.245437	10.027902	0.360346
-269.662626	18.606327	0.365350
-273.013560	18.912727	0.370355
-277.316250	13.080742	0.375360
-280.862680	13.125053	0.380365
-285.127541	12.911898	0.385370
-288.909930	12.730541	0.390374
-292.263723	15.669293	0.395379
-296.416943	23.438022	0.400384
-300.139559	14.115232	0.405389
-303.564715	16.496126	0.410394
-307.690242	18.410101	0.415398
-311.281923	11.032841	0.420403
-314.844284	19.456309	0.425408
-318.788980	24.993570	0.430413
-322.035855	19.120846	0.435418
-326.148814	15.139921	0.440422
-329.834321	13.405672	0.445427
-333.682352	10.462652	0.450432
-337.602506	9.101759	0.455437
-341.493644	9.308421	0.460442
-345.288141	23.835378	0.465446
-348.641315	10.885132	0.470451
-352.475043	15.308773	0.475456
-356.116508	17.837813	0.480461
-359.948060	11.944955	0.485466
-364.408588	18.012484	0.490470
-368.092649	12.059823	0.495475
-371.697284	12.146676	0.500480
-374.997686	12.186537	0.505485
-378.608090	4.150074	0.510490
-382.701296	9.726911	0.515494
-385.890184	9.100871	0.520499
-390.152113	10.907458	0.525504
-394.065952	8.697272	0.530509
-397.679029	14.096550	0.535514
-401.734288	9.649242	0.540518
-405.236788	5.873752	0.545523
-409.337066	16.092614	0.550528
-412.859234	13.028307	0.555533
-416.202217	6.899840	0.560538
-420.488677	21.666303	0.565542
-423.929636	-4.758695	0.570547
-427.921923	9.325299	0.575552
-431.605271	16.063608	0.580557
-435.340566	8.580172	0.585562
-439.304361	22.896183	0.590566
-443.073539	9.523674	0.595571
-446.410840	18.018615	0.600576
-450.392088	15.204290	0.605581
-453.951672	5.622342	0.610586
-457.818530	9.865360	0.615590
-461.806916	8.602299	0.620595
-465.957922	15.131498	0.625600
-469.395485	16.022849	0.630605
-472.764960	6.949873	0.635610
-476.597857	16.916413	0.640614
-480.308166	10.286900	0.645619
-484.228820	24.996625	0.650624
-488.227074	12.990113	0.655629
-492.054061	11.024831	0.660634
-495.920295	13.604170	0.665638
-499.197216	7.365929	0.670643
-503.252936	24.372734	0.675648
-506.496604	13.329073	0.680653
-509.992228	12.020505	0.685658
-514.068817	24.438700	0.690662
-517.989490	8.906496	0.695667
-522.045853	21.663660	0.700672
-525.541581	5.242030	0.705677
-529.443323	6.846257	0.710682
-533.377880	16.734505	0.715686
-536.610870	6.576988	0.720691
-540.735795	9.063682	0.725696
-544.474107	9.731951	0.730701
-548.274148	13.533944	0.735706
-552.026393	11.170478	0.740710
-555.823953	6.657046	0.745715
-559.662440	11.707801	0.750720
-563.235259	14.532105	0.755725
-567.080192	13.777724	0.760730
-570.823796	21.180283	0.765734
-574.662476	10.072508	0.770739
-578.347291	7.037588	0.775744
-581.740003	13.040580	0.780749
-585.701172	10.622236	0.785754
-589.589911	18.540003	0.790758
-593.395564	13.294661	0.795763
-597.209682	6.368119	0.800768
-600.711029	4.019842	0.805773
-604.408514	4.192842	0.810778
-608.187068	11.156348	0.815782
-611.962997	4.524920	0.820787
-616.123363	11.785973	0.825792
-620.203327	3.839109	0.830797
-623.454300	10.798770	0.835802
-627.411492	4.311443	0.840806
-630.788225	12.530655	0.845811
-634.848624	6.223828	0.850816
-638.160987	5.259898	0.855821
-642.080470	7.139947	0.860826
-646.142583	3.974613	0.865830
-649.804213	12.952133	0.870835
-653.506398	13.837145	0.875840
-657.360839	9.586851	0.880845
-661.190575	13.322803	0.885850
-665.079343	16.196165	0.890854
-668.523869	11.263820	0.895859
-672.638018	16.082840	0.900864
-676.152020	11.587373	0.905869
-679.800355	12.724011	0.910874
-683.699603	1.774340	0.915878
-687.329001	5.107747	0.920883
-691.061797	8.791986	0.925888
-694.894896	10.596818	0.930893
-698.317430	1.677743	0.935898
-702.367452	8.572810	0.940902
-705.970482	8.205765	0.945907
-709.969099	13.359612	0.950912
-713.536729	12.236313	0.955917
-717.416723	12.787151	0.960922
-721.536379	8.782769	0.965926
-725.245301	8.363291	0.970931
-728.973302	11.351408	0.975936
-732.346722	-0.937425	0.980941
-736.322283	7.196283	0.985946
-740.077132	7.366047	0.990950
-743.644871	2.797275	0.995955
-747.797489	6.034625	1.000960
-751.428088	12.730282	1.005965
-754.846704	1.402734	1.010970
-759.249346	12.602433	1.015974
-762.497759	12.491025	1.020979
-766.538825	23.565148	1.025984
-770.164139	10.846707	1.030989
-774.040321	15.566365	1.035994
-777.706267	1.214458	1.040998
-781.316577	6.557084	1.046003
-785.495475	9.943775	1.051008
-788.737553	7.357227	1.056013
-792.337767	5.206386	1.061018
-796.417278	13.673765	1.066022
-800.221063	8.844775	1.071027
-804.348480	7.230791	1.076032
-808.048465	7.921734	1.081037
-811.630952	15.158552	1.086042
-815.619323	9.815060	1.091046
-818.786211	-4.170280	1.096051
-822.530958	3.921937	1.101056
-826.421595	7.320965	1.106061
-829.973477	-0.501779	1.111066
-834.167527	6.290374	1.116070
-837.768779	0.339434	1.121075
-842.250148	2.085712	1.126080
-845.466623	3.196143	1.131085
-848.812358	14.703267	1.136090
-852.547478	5.888014	1.141094
-856.602639	-0.075486	1.146099
-860.599973	5.425320	1.151104
-864.301558	4.922890	1.156109
-868.108362	7.756668	1.161114
-871.893196	6.772412	1.166118
-875.470603	0.497608	1.171123
-879.066693	8.036307	1.176128
-882.740252	2.505415	1.181133
-886.687336	7.572467	1.186138
-890.805504	12.078695	1.191142
-894.523790	4.046120	1.196147
-898.009554	12.442390	1.201152
-901.702918	10.905834	1.206157
-905.502175	8.889490	1.211162
-909.360683	11.398874	1.216166
-912.859823	1.631392	1.221171
-916.675665	15.492392	1.226176
-920.799323	11.492161	1.231181
-924.516517	5.585125	1.236186
-928.509957	14.535684	1.241190
-931.715070	7.852943	1.246195
-935.435943	14.109158	1.251200
-939.275135	8.256345	1.256205
-942.964974	1.988588	1.261210
-946.848119	14.281915	1.266214
-950.388531	5.188120	1.271219
-954.292547	9.193449	1.276224
-958.291024	12.564206	1.281229
-962.135981	9.183359	1.286234
-965.927776	9.595926	1.291238
-969.489709	5.870222	1.296243
-973.553151	4.727265	1.301248
-977.375643	8.263869	1.306253
-980.284704	-1.153180	1.311258
-984.726504	0.735269	1.316262
-988.273187	10.076507	1.321267
-992.343513	14.184186	1.326272
-996.023843	17.814778	1.331277
-999.717134	8.319746	1.336282
-1003.556015	15.941611	1.341286
-1006.651232	-0.713567	1.346291
-1011.200885	14.800830	1.351296
-1014.574171	11.283136	1.356301
-1018.403785	3.110885	1.361306
-1022.219321	16.457924	1.366310
-1025.992510	-3.703047	1.371315
-1029.852495	9.067653	1.376320
-1033.370421	4.800442	1.381325
-1037.026102	8.253693	1.386330
-1041.048877	8.531444	1.391334
-1044.746546	13.773321	1.396339
-1048.407501	7.434886	1.401344
-1052.328713	10.405524	1.406349
-1056.120079	8.189477	1.411354
-1060.390736	12.004473	1.416358
-1063.167028	11.537277	1.421363
-1067.299678	17.462181	1.426368
-1070.859397	15.951824	1.431373
-1074.630784	3.813914	1.436378
-1078.963720	10.324364	1.441382
-1082.346295	7.798551	1.446387
-1086.340021	18.662190	1.451392
-1090.101904	12.327350	1.456397
-1093.514356	8.002360	1.461402
-1097.480878	6.211780	1.466406
-1100.910812	5.527504	1.471411
-1104.904128	8.136038	1.476416
-1108.687113	7.815747	1.481421
-1112.347108	4.071263	1.486426
-1116.375132	9.869127	1.491430
-1119.651274	2.332307	1.496435
-1123.924245	15.364758	1.501440
-1127.742358	4.574780	1.506445
-1130.990429	-3.625654	1.511450
-1134.995712	12.476783	1.516454
-1138.671253	-17.706576	1.521459
-1142.559686	8.084543	1.526464
-1146.710649	15.269299	1.531469
-1150.236840	6.572508	1.536474
-1153.806403	7.714620	1.541478
-1157.000578	-5.608275	1.546483
-1161.002784	10.744434	1.551488
-1165.290684	10.780976	1.556493
-1169.171285	11.340541	1.561498
-1172.991310	9.195502	1.566502
-1175.940717	8.123804	1.571507
-1180.055144	13.989215	1.576512
-1183.858614	9.184473	1.581517
-1187.836438	10.593804	1.586522
-1191.821400	15.705264	1.591526
-1195.125682	22.147524	1.596531
-1198.795988	12.292770	1.601536
-1202.056208	13.128424	1.606541
-1206.139770	6.402148	1.611546
-1210.228244	24.364571	1.616550
-1214.284975	9.041498	1.621555
-1217.883154	1.535857	1.626560
-1221.455602	12.414293	1.631565
-1225.350205	7.619474	1.636570
-1229.107242	11.240623	1.641574
-1232.766145	13.622401	1.646579
-1236.676067	15.533441	1.651584
-1240.490141	2.637861	1.656589
-1243.839096	-2.826116	1.661594
-1248.077203	10.054311	1.666598
-1251.319279	-3.697577	1.671603
-1255.717073	17.862425	1.676608
-1259.278150	11.935690	1.681613
-1262.680783	-0.264053	1.686618
-1266.571060	8.594847	1.691622
-1270.199838	1.070536	1.696627
-1274.354928	12.417596	1.701632
-1278.311463	16.364054	1.706637
-1281.519836	16.013579	1.711642
-1285.524402	9.129731	1.716646
-1288.975743	2.472728	1.721651
-1292.846517	1.275843	1.726656
-1296.680534	10.261400	1.731661
-1300.436493	0.909373	1.736666
-1304.757226	16.598959	1.741670
-1307.995435	5.315951	1.746675
-1311.736046	13.370407	1.751680
-1315.566357	7.892120	1.756685
-1319.065124	8.679391	1.761690
-1322.914300	21.180744	1.766694
-1326.751689	8.705345	1.771699
-1331.069394	23.621820	1.776704
-1334.760582	19.870070	1.781709
-1338.015358	10.554568	1.786714
-1341.670205	7.995456	1.791718
-1345.472512	6.481782	1.796723
-1349.366713	14.264426	1.801728
-1353.073354	5.566888	1.806733
-1356.702176	6.807103	1.811738
-1360.878730	17.358262	1.816742
-1364.451020	-7.131274	1.821747
-1368.315236	-3.756092	1.826752
-1371.900782	9.187229	1.831757
-1375.259614	9.472807	1.836762
-1379.674286	13.385547	1.841766
-1383.428662	5.449459	1.846771
-1387.174353	7.624606	1.851776
-1391.029369	7.858761	1.856781
-1394.638111	14.395761	1.861786
-1398.034571	8.203209	1.866790
-1401.648876	2.815065	1.871795
-1405.863170	4.773540	1.876800
-1409.878482	11.752531	1.881805
-1413.309060	11.704311	1.886810
-1417.362044	10.497386	1.891814
-1420.825366	2.040120	1.896819
-1424.633464	5.693406	1.901824
-1428.339702	10.743287	1.906829
-1431.887193	6.328475	1.911834
-1435.968335	20.760989	1.916838
-1439.482376	12.171524	1.921843
-1443.243232	8.301805	1.926848
-1447.324003	15.449031	1.931853
-1450.862058	10.928662	1.936858
-1454.612191	8.348721	1.941862
-1458.164901	2.050402	1.946867
-1462.643229	21.851223	1.951872
-1466.080567	6.322230	1.956877
-1469.841900	10.479015	1.961882
-1473.686894	12.799508	1.966886
-1477.088955	1.383735	1.971891
-1481.091936	12.618477	1.976896
-1484.862319	17.819063	1.981901
-1488.260030	3.925310	1.986906
-1492.607325	12.679568	1.991910
-1495.912867	11.282129	1.996915
-1499.944894	22.689114	2.006912
-1501.255975	13.258592	2.016909
-1498.479015	15.613651	2.026906
-1495.694383	14.951763	2.036902
-1493.531428	17.433575	2.046899
-1491.781055	13.894755	2.056896
-1489.396067	13.307925	2.066893
-1487.822010	10.649955	2.076890
-1485.885729	6.508225	2.086886
-1484.160014	7.654831	2.096883
-1482.147511	6.090313	2.106880
-1480.515427	8.090316	2.116877
-1477.902094	3.642812	2.126874
-1476.052711	3.683330	2.136870
-1474.934703	0.158946	2.146867
-1472.822297	-1.716818	2.156864
-1470.892492	3.091767	2.166861
-1468.729999	4.498436	2.176858
-1466.995753	5.247382	2.186854
-1465.110116	2.912159	2.196851
-1463.309499	10.223487	2.206848
-1461.386912	9.162847	2.216845
-1459.094370	3.554125	2.226842
-1457.406716	4.541060	2.236838
-1455.752900	6.956013	2.246835
-1453.689327	1.707637	2.256832
-1452.156801	6.699850	2.266829
-1449.911366	5.810151	2.276826
-1447.958193	0.086837	2.286822
-1445.985334	-2.567066	2.296819
-1444.491151	9.566391	2.306816
-1442.477776	5.224461	2.316813
-1440.595290	8.228061	2.326810
-1438.478067	3.593198	2.336806
-1436.861084	-1.070511	2.346803
-1434.796005	7.692146	2.356800
-1433.044451	9.704634	2.366797
-1431.290772	-4.847575	2.376794
-1429.536231	6.099495	2.386790
-1427.611295	8.357378	2.396787
-1425.485576	2.137518	2.406784
-1423.583025	9.203618	2.416781
-1421.758171	-8.337806	2.426778
-1419.836885	5.718290	2.436774
-1418.097139	4.039606	2.446771
-1416.063148	10.486261	2.456768
-1414.228261	1.031995	2.466765
-1412.405322	1.203111	2.476762
-1410.644863	2.374209	2.486758
-1408.649168	4.963404	2.496755
-1406.679128	-0.991521	2.506752
-1404.921631	6.007820	2.516749
-1402.892978	-4.688483	2.526746
-1401.024101	0.374649	2.536742
-1399.296122	5.968752	2.546739
-1397.023004	9.620361	2.556736
-1395.666771	8.933071	2.566733
-1393.723465	6.064472	2.576730
-1391.055558	4.470893	2.586726
-1390.089706	5.030288	2.596723
-1387.987318	5.919300	2.606720
-1386.144518	8.231421	2.616717
-1384.144386	5.912667	2.626714
-1382.496754	7.007116	2.636710
-1380.459542	2.156170	2.646707
-1378.470517	10.719487	2.656704
-1376.581882	11.966406	2.666701
-1374.914890	9.443629	2.676698
-1372.913593	9.286230	2.686694
-1370.742655	10.230599	2.696691
-1368.804448	12.026946	2.706688
-1367.560119	15.789597	2.716685
-1365.542264	15.072197	2.726682
-1363.249048	18.428527	2.736678
-1361.750958	13.985995	2.746675
-1360.076181	9.709388	2.756672
-1357.835088	16.707146	2.766669
-1355.969972	9.018039	2.776666
-1354.040212	10.567861	2.786662
-1352.259040	7.178945	2.796659
-1350.494675	9.811539	2.806656
-1348.567554	15.490649	2.816653
-1346.779156	12.230051	2.826650
-1344.272957	11.213450	2.836646
-1342.686969	7.879469	2.846643
-1341.092460	9.929799	2.856640
-1339.067098	3.359768	2.866637
-1337.280579	-1.717848	2.876634
-1335.558901	5.028342	2.886630
-1333.517050	0.402477	2.896627
-1331.575774	4.516208	2.906624
-1329.782791	1.985927	2.916621
-1327.755827	7.881171	2.926618
-1325.648870	3.445412	2.936614
-1324.059643	-3.219000	2.946611
-1322.447117	9.648751	2.956608
-1320.530476	7.507622	2.966605
-1318.175268	10.756181	2.976602
-1316.614473	7.123097	2.986598
-1314.726187	-1.854919	2.996595
-1312.894803	2.349047	3.006592
-1311.217734	7.774532	3.016589
-1309.029477	4.814691	3.026586
-1307.012401	6.716885	3.036582
-1305.226180	7.658157	3.046579
-1303.421968	11.830168	3.056576
-1301.624089	4.931847	3.066573
-1299.706938	4.939555	3.076570
-1297.659123	6.783155	3.086566
-1296.003259	9.322634	3.096563
-1293.947593	7.890312	3.106560
-1292.056654	7.592754	3.116557
-1290.197259	0.316711	3.126554
-1288.524527	9.121784	3.136550
-1286.521190	-2.985087	3.146547
-1285.095500	4.989544	3.156544
-1282.765536	3.645960	3.166541
-1281.009281	10.315612	3.176538
-1278.876874	1.410651	3.186534
-1276.845033	9.701954	3.196531
-1275.278508	1.825438	3.206528
-1273.318636	3.507874	3.216525
-1271.751917	1.495417	3.226522
-1269.733750	1.441195	3.236518
-1267.670504	0.145049	3.246515
-1266.237020	3.948534	3.256512
-1264.067991	6.950635	3.266509
-1261.973734	1.455934	3.276506
-1260.092431	4.308300	3.286502
-1258.559685	6.501202	3.296499
-1256.573782	10.571544	3.306496
-1254.544028	12.828591	3.316493
-1252.957164	3.802539	3.326490
-1251.004817	6.450916	3.336486
-1248.839679	1.126458	3.346483
-1246.987925	6.400883	3.356480
-1245.376659	14.165853	3.366477
-1243.464510	-0.091090	3.376474
-1241.299635	9.803661	3.386470
-1239.468244	3.447905	3.396467
-1238.010256	8.395360	3.406464
-1235.958449	9.382604	3.416461
-1234.072641	8.441718	3.426458
-1232.106439	3.951197	3.436454
-1230.230935	12.616505	3.446451
-1228.278101	6.535000	3.456448
-1226.528705	13.791575	3.466445
-1224.539746	11.566319	3.476442
-1222.667075	6.413418	3.486438
-1220.894809	3.515488	3.496435
-1218.961391	-2.180802	3.506432
-1217.374540	4.122859	3.516429
-1215.089450	4.425437	3.526426
-1213.417931	-4.123091	3.536422
-1211.516167	4.187508	3.546419
-1209.578754	-3.685159	3.556416
-1207.898403	6.189264	3.566413
-1205.675647	3.680303	3.576410
-1203.912619	6.610062	3.586406
-1201.938209	2.591928	3.596403
-1200.310043	0.261797	3.606400
-1198.458911	2.692735	3.616397
-1196.457359	-0.870273	3.626394
-1194.259880	2.312076	3.636390
-1192.786010	5.940204	3.646387
-1190.822845	0.938634	3.656384
-1189.278712	3.016079	3.666381
-1187.242876	9.906332	3.676378
-1185.004906	0.752456	3.686374
-1183.349523	3.847873	3.696371
-1181.449371	0.664253	3.706368
-1179.526328	7.951499	3.716365
-1177.503396	13.907530	3.726362
-1175.994093	5.604444	3.736358
-1174.077223	1.644485	3.746355
-1171.850632	10.086305	3.756352
-1170.285529	6.351575	3.766349
-1168.129019	5.241116	3.776346
-1166.343652	0.732215	3.786342
-1164.423374	11.341958	3.796339
-1162.865069	5.854143	3.806336
-1160.723287	2.862400	3.816333
-1158.893579	6.935714	3.826330
-1157.413674	2.050963	3.836326
-1154.999184	-1.807021	3.846323
-1153.134351	1.611742	3.856320
-1151.525553	8.856135	3.866317
-1149.590774	1.498659	3.876314
-1147.781806	0.656975	3.886310
-1145.563275	3.727058	3.896307
-1143.567739	-1.638066	3.906304
-1142.373870	3.934328	3.916301
-1139.946298	3.865244	3.926298
-1138.472403	2.327190	3.936294
-1136.723906	3.094632	3.946291
-1134.671616	3.428218	3.956288
-1132.624753	7.155766	3.966285
-1130.498877	8.311251	3.976282
-1128.859374	14.603402	3.986278
-1127.010136	11.746908	3.996275
-1125.249850	13.191408	4.006272
-1123.323992	16.305180	4.016269
-1121.292511	15.563706	4.026266
-1119.568423	4.884756	4.036262
-1117.424380	4.466324	4.046259
-1115.427284	3.514045	4.056256
-1113.872794	1.066287	4.066253
-1112.241775	10.782898	4.076250
-1110.205767	8.333900	4.086246
-1108.437655	1.937835	4.096243
-1106.469482	5.985885	4.106240
-1104.387669	8.695782	4.116237
-1102.592199	13.431452	4.126234
-1100.818912	9.117156	4.136230
-1098.780193	5.281444	4.146227
-1096.965685	10.574588	4.156224
-1095.222356	10.288171	4.166221
-1093.353221	10.976350	4.176218
-1091.300145	5.092070	4.186214
-1089.096452	2.875208	4.196211
-1087.811792	-0.213040	4.206208
-1086.042862	3.607956	4.216205
-1083.754724	7.803787	4.226202
-1081.810342	8.217837	4.236198
-1080.258830	7.251602	4.246195
-1078.315470	6.855834	4.256192
-1076.128989	10.317949	4.266189
-1074.539528	4.428896	4.276186
-1072.738443	12.286791	4.286182
-1070.623044	1.565807	4.296179
-1068.626389	-3.693649	4.306176
-1067.098067	2.652643	4.316173
-1065.238141	3.283897	4.326170
-1063.309978	0.637456	4.336166
-1061.247213	1.561526	4.346163
-1059.450822	5.837616	4.356160
-1057.571298	1.353205	4.366157
-1055.686813	6.482034	4.376154
-1053.939680	7.401333	4.386150
-1052.327548	1.759717	4.396147
-1049.932045	5.317894	4.406144
-1048.176780	5.021709	4.416141
-1046.364588	2.726982	4.426138
-1044.350789	0.145806	4.436134
-1042.419126	0.004565	4.446131
-1040.688310	1.513842	4.456128
-1038.816421	7.802047	4.466125
-1037.180369	-0.832277	4.476122
-1035.049936	4.408807	4.486118
-1033.357560	-1.602466	4.496115
-1031.404956	2.182881	4.506112
-1029.554592	4.672501	4.516109
-1027.379822	-0.913826	4.526106
-1025.698881	5.673346	4.536102
-1023.770688	7.560007	4.546099
-1021.790255	-0.074670	4.556096
-1020.163210	5.270623	4.566093
-1018.052631	-0.475953	4.576090
-1016.491485	2.239930	4.586086
-1014.180555	-0.541897	4.596083
-1012.352137	-4.707053	4.606080
-1010.823290	-1.780742	4.616077
-1009.268688	7.324499	4.626074
-1006.738422	-1.598080	4.636070
-1004.888026	2.612576	4.646067
-1003.195791	-1.352376	4.656064
-1001.190196	-1.446986	4.666061
-999.507781	4.656821	4.676058
-997.844479	11.671568	4.686054
-995.737020	7.553374	4.696051
-993.432925	7.155248	4.706048
-991.987702	5.257138	4.716045
-990.286652	1.628673	4.726042
-987.867563	1.766363	4.736038
-986.303164	1.341276	4.746035
-984.647301	4.016772	4.756032
-982.563397	12.718448	4.766029
-980.762823	11.136142	4.776026
-978.785230	16.152258	4.786022
-976.724106	5.782649	4.796019
-974.945023	8.800021	4.806016
-973.263681	3.627377	4.816013
-971.309309	8.587211	4.826010
-969.174366	-1.085257	4.836006
-967.243372	2.750970	4.846003
-965.772122	2.175006	4.856000
-963.932990	4.822789	4.865997
-961.888414	6.457212	4.875994
-960.230031	4.577139	4.885990
-958.067745	1.392826	4.895987
-956.049765	3.160978	4.905984
-954.473738	7.699756	4.915981
-952.643943	0.315005	4.925978
-950.692924	3.508581	4.935974
-948.647489	0.502433	4.945971
-946.768854	-0.137083	4.955968
-944.987430	1.193650	4.965965
-943.208174	5.848358	4.975962
-941.477096	2.914587	4.985958
-939.408246	4.968299	4.995955
-937.398794	5.449432	5.005952
-935.385527	-1.022028	5.015949
-933.751458	11.252089	5.025946
-932.289972	10.178769	5.035942
-930.020553	6.653670	5.045939
-928.040185	2.560593	5.055936
-926.195526	-1.112895	5.065933
-924.452514	5.101280	5.075930
-922.387740	0.312618	5.085926
-920.458867	1.117697	5.095923
-918.678783	5.039674	5.105920
-917.039869	5.415863	5.115917
-915.076980	12.229619	5.125914
-913.005915	7.915212	5.135910
-911.167135	2.483756	5.145907
-909.326236	4.878674	5.155904
-907.609713	5.149304	5.165901
-905.665124	8.141847	5.175898
-903.901902	8.603958	5.185894
-901.541191	4.385354	5.195891
-900.291515	9.533711	5.205888
-897.981897	11.956328	5.215885
-896.154130	14.986505	5.225882
-894.425352	10.401580	5.235878
-892.593219	10.560582	5.245875
-890.369356	11.146421	5.255872
-888.741931	8.709250	5.265869
-886.669931	12.183536	5.275866
-884.883074	11.452955	5.285862
-883.243631	10.466474	5.295859
-881.471294	4.922506	5.305856
-879.558989	10.997551	5.315853
-877.546951	11.443587	5.325850
-875.304678	5.311342	5.335846
-873.724045	6.841598	5.345843
-871.717466	5.922744	5.355840
-870.011396	13.023911	5.365837
-868.340280	12.007114	5.375834
-866.291142	11.514085	5.385830
-864.155372	10.596688	5.395827
-862.355000	4.536680	5.405824
-860.500613	12.016769	5.415821
-858.680684	15.518748	5.425818
-856.876321	13.309097	5.435814
-854.810297	14.403353	5.445811
-853.194662	12.184402	5.455808
-851.371217	11.740098	5.465805
-849.394311	13.529121	5.475802
-847.285454	6.142460	5.485798
-845.560439	9.487519	5.495795
-843.677677	9.801095	5.505792
-841.896508	7.603057	5.515789
-839.858464	9.893886	5.525786
-837.821187	23.177305	5.535782
-835.912077	17.974652	5.545779
-834.606973	13.478020	5.555776
-832.333710	16.557032	5.565773
-830.521356	21.144968	5.575770
-828.985884	14.918907	5.585766
-826.751399	15.771526	5.595763
-824.954198	17.762979	5.605760
-823.195334	15.521152	5.615757
-821.195350	12.353428	5.625754
-819.078189	18.769988	5.635750
-817.266730	6.659383	5.645747
-815.528071	11.960149	5.655744
-813.659303	12.140198	5.665741
-811.899978	19.218692	5.675738
-809.848590	13.027016	5.685734
-808.029660	13.028723	5.695731
-806.111746	13.505655	5.705728
-804.299981	13.439037	5.715725
-802.615904	12.436003	5.725722
-800.673383	19.778904	5.735718
-798.498534	12.684884	5.745715
-796.800737	14.246991	5.755712
-794.722369	7.902598	5.765709
-792.962103	18.846162	5.775706
-791.124447	18.969624	5.785702
-789.391938	15.784679	5.795699
-787.586143	15.338508	5.805696
-785.344834	16.737962	5.815693
-783.548136	13.040665	5.825690
-781.826758	10.975383	5.835686
-779.861113	11.896279	5.845683
-778.139657	9.788357	5.855680
-776.077239	23.178345	5.865677
-774.608437	17.438227	5.875674
-772.536324	16.224775	5.885670
-770.481439	9.363109	5.895667
-768.524759	16.792194	5.905664
-766.513653	11.527505	5.915661
-764.627680	19.757358	5.925658
-763.431981	19.433978	5.935654
-761.201869	11.530642	5.945651
-759.216897	10.561652	5.955648
-757.176822	9.337545	5.965645
-755.421896	19.372535	5.975642
-753.660766	16.375670	5.985638
-751.829420	11.014987	5.995635
-750.160071	10.132763	6.005632
-748.000126	11.019475	6.015629
-746.078143	12.818943	6.025626
-744.356396	13.407802	6.035622
-742.120353	14.151307	6.045619
-740.337632	20.316661	6.055616
-738.651392	6.304565	6.065613
-736.985736	13.728083	6.075610
-734.964931	17.766473	6.085606
-732.978186	12.283075	6.095603
-731.059101	10.250969	6.105600
-728.990177	17.388999	6.115597
-727.364196	14.146912	6.125594
-725.666973	18.014395	6.135590
-723.894871	19.815731	6.145587
-721.563600	17.539342	6.155584
-719.986087	16.902338	6.165581
-717.989489	12.749989	6.175578
-716.146891	15.588471	6.185574
-713.912905	6.735625	6.195571
-712.474961	8.446687	6.205568
-710.401333	7.690935	6.215565
-708.543509	5.982843	6.225562
-706.729048	12.496828	6.235558
-704.833338	18.329948	6.245555
-702.938520	10.871817	6.255552
-700.939574	13.355331	6.265549
-699.342689	19.245682	6.275546
-697.564495	16.042448	6.285542
-695.475855	12.489612	6.295539
-693.550900	19.551210	6.305536
-691.647280	19.815786	6.315533
-689.612647	13.784775	6.325530
-688.022587	9.421102	6.335526
-686.085934	14.841911	6.345523
-684.128574	8.516943	6.355520
-682.326268	13.165023	6.365517
-680.447194	12.928273	6.375514
-678.413907	14.102127	6.385510
-676.663132	17.383202	6.395507
-675.140627	17.689742	6.405504
-673.000463	10.074010	6.415501
-671.131280	12.788281	6.425498
-669.067808	16.194658	6.435494
-667.189924	21.727507	6.445491
-665.306925	15.880215	6.455488
-663.686014	21.544126	6.465485
-661.541883	19.225066	6.475482
-660.021530	15.718851	6.485478
-658.103240	20.222107	6.495475
-655.918085	17.102297	6.505472
-654.190415	14.230847	6.515469
-652.257373	14.880748	6.525466
-650.548082	25.238908	6.535462
-648.460723	16.218490	6.545459
-646.567106	3.270667	6.555456
-644.796006	14.373676	6.565453
-642.982522	13.945332	6.575450
-641.030589	13.166453	6.585446
-639.268709	15.091064	6.595443
-637.282443	8.906774	6.605440
-635.467168	16.947513	6.615437
-633.409679	10.698162	6.625434
-631.587780	10.009539	6.635430
-630.019801	16.926124	6.645427
-627.962639	11.303664	6.655424
-625.795130	5.082533	6.665421
-624.091179	5.699585	6.675418
-622.427109	16.567086	6.685414
-620.123375	9.826831	6.695411
-618.852393	4.029990	6.705408
-616.626938	10.667858	6.715405
-614.901032	8.821442	6.725402
-613.149451	2.399934	6.735398
-610.953932	11.680976	6.745395
-608.737553	12.683536	6.755392
-607.297379	9.131743	6.765389
-605.390357	18.432045	6.775386
-603.586756	24.024184	6.785382
-601.937485	22.199492	6.795379
-599.670077	17.160825	6.805376
-597.722825	14.674329	6.815373
-596.059136	18.064115	6.825370
-594.263972	17.040322	6.835366
-592.389559	14.797569	6.845363
-590.297914	17.861627	6.855360
-588.383591	18.932987	6.865357
-586.801831	11.895998	6.875354
-584.706856	14.953212	6.885350
-582.924632	9.275238	6.895347
-580.746989	12.126620	6.905344
-579.118887	7.292733	6.915341
-577.315336	13.521205	6.925338
-575.367841	22.204026	6.935334
-573.616017	17.454585	6.945331
-571.443369	13.411596	6.955328
-569.848959	4.673674	6.965325
-567.674246	15.974377	6.975322
-566.098989	3.247987	6.985318
-564.315562	14.516462	6.995315
-562.282447	13.839941	7.005312
-560.210434	15.536652	7.015309
-558.539686	16.320106	7.025306
-556.626118	16.802672	7.035302
-554.564216	15.578407	7.045299
-552.977298	11.156899	7.055296
-550.926501	20.720071	7.065293
-549.066621	18.171781	7.075290
-547.369900	11.680130	7.085286
-545.270976	14.629382	7.095283
-543.429339	12.887686	7.105280
-541.672442	14.588959	7.115277
-540.084927	10.729462	7.125274
-537.701741	20.637443	7.135270
-535.901689	18.343454	7.145267
-534.270843	15.113346	7.155264
-532.101295	11.869825	7.165261
-530.164203	11.619190	7.175258
-528.500795	15.534853	7.185254
-526.640926	17.170744	7.195251
-524.700787	18.555396	7.205248
-522.879031	14.292184	7.215245
-520.694490	14.360449	7.225242
-519.018266	19.879844	7.235238
-517.330598	17.897499	7.245235
-515.365472	15.954523	7.255232
-513.209785	7.229613	7.265229
-511.803763	16.594229	7.275226
-510.030842	16.732985	7.285222
-507.684471	9.723919	7.295219
-506.098284	15.862433	7.305216
-504.047817	14.804246	7.315213
-502.091598	15.630566	7.325210
-500.247076	21.483092	7.335206
-498.557612	14.700527	7.345203
-496.557612	20.416120	7.355200
-494.596946	17.128624	7.365197
-492.754373	17.518371	7.375194
-490.877851	17.994275	7.385190
-489.256985	24.618314	7.395187
-486.980069	20.438745	7.405184
-485.349627	13.851929	7.415181
-483.933406	16.806063	7.425178
-481.455558	8.688140	7.435174
-479.516790	13.180381	7.445171
-477.802870	12.663854	7.455168
-475.860131	14.900754	7.465165
-473.922617	15.291142	7.475162
-472.192101	14.261975	7.485158
-470.331620	17.427795	7.495155
-468.199670	13.928232	7.505152
-466.574559	10.872767	7.515149
-464.388967	16.925060	7.525146
-463.044620	16.322303	7.535142
-461.023429	15.289354	7.545139
-459.164043	14.226984	7.555136
-457.441089	16.372685	7.565133
-455.230279	13.878948	7.575130
-453.322880	16.222562	7.585126
-451.320562	14.584747	7.595123
-449.541802	7.135858	7.605120
-447.819077	13.500501	7.615117
-446.101224	18.697518	7.625114
-443.751617	23.259973	7.635110
-442.119318	20.815999	7.645107
-440.432893	18.560751	7.655104
-438.434367	20.518777	7.665101
-436.462959	20.687469	7.675098
-434.652594	18.396643	7.685094
-432.958100	17.553254	7.695091
-430.914629	17.816232	7.705088
-428.960973	16.846199	7.715085
-427.047515	21.634632	7.725082
-425.343825	16.821926	7.735078
-423.202432	17.309271	7.745075
-421.616774	24.598976	7.755072
-419.658585	16.974610	7.765069
-417.736467	19.890634	7.775066
-415.548018	15.507365	7.785062
-414.225653	25.674878	7.795059
-412.362038	16.770895	7.805056
-410.339827	16.618869	7.815053
-408.133830	12.823325	7.825050
-406.653064	12.494077	7.835046
-404.630148	21.221852	7.845043
-402.848391	20.015606	7.855040
-400.965630	13.019083	7.865037
-399.068107	5.777051	7.875034
-396.899671	8.885863	7.885030
-395.304974	14.011004	7.895027
-393.157756	16.239007	7.905024
-391.503043	11.472040	7.915021
-389.700463	19.475543	7.925018
-387.755773	14.629119	7.935014
-385.843768	15.183123	7.945011
-384.007453	16.360261	7.955008
-382.088433	17.412092	7.965005
-379.936307	17.443030	7.975002
-378.543597	24.643575	7.984998
-376.902707	17.789895	7.994995
-374.601355	13.936524	8.004992
-372.573059	18.954559	8.014989
-370.789169	18.865880	8.024986
-369.044038	16.187626	8.034982
-366.974184	19.724310	8.044979
-365.285905	22.276664	8.054976
-363.354184	24.136475	8.064973
-361.412337	13.153215	8.074970
-359.692043	13.938373	8.084966
-357.493703	14.459317	8.094963
-355.843830	22.621440	8.104960
-353.828309	6.944893	8.114957
-352.249439	14.764669	8.124954
-350.172193	13.643917	8.134950
-348.402178	9.272249	8.144947
-346.399729	6.211883	8.154944
-344.676442	10.127594	8.164941
-342.639773	5.623361	8.174938
-340.879653	10.262661	8.184934
-338.980979	6.288877	8.194931
-337.214650	7.731432	8.204928
-335.117560	8.819607	8.214925
-333.390498	4.787963	8.224922
-331.135697	10.036711	8.234918
-329.578078	12.425214	8.244915
-327.902541	15.382256	8.254912
-325.952841	6.802486	8.264909
-324.157738	14.016190	8.274906
-322.354166	19.482247	8.284902
-320.054234	16.789668	8.294899
-318.190415	15.758277	8.304896
-316.420783	12.626153	8.314893
-314.662739	14.812146	8.324890
-312.546263	12.857803	8.334886
-310.730995	20.489877	8.344883
-308.927556	14.164496	8.354880
-307.051436	13.151675	8.364877
-305.284395	19.084626	8.374874
-303.179982	15.996963	8.384870
-301.313625	16.397271	8.394867
-299.652257	15.594000	8.404864
-297.865616	15.309148	8.414861
-295.951503	12.220290	8.424858
-293.944148	10.314960	8.434854
-292.082402	14.219663	8.444851
-290.276734	13.502310	8.454848
-288.102751	7.280427	8.464845
-286.491958	14.602530	8.474842
-284.452317	15.570448	8.484838
-282.513991	12.929311	8.494835
-280.808069	10.060012	8.504832
-278.998075	14.077196	8.514829
-276.829070	8.314007	8.524826
-275.328532	7.309058	8.534822
-273.261773	9.204227	8.544819
-271.579888	8.555593	8.554816
-269.666760	11.226860	8.564813
-267.854413	14.368949	8.574810
-265.597532	13.279594	8.584807
-263.816607	12.539368	8.594803
-261.881426	11.444524	8.604800
-260.035442	15.364401	8.614797
-258.310148	14.290430	8.624794
-256.303998	20.003678	8.634791
-254.416227	20.907443	8.644787
-252.789337	16.756050	8.654784
-250.639367	11.018025	8.664781
-248.773549	13.376338	8.674778
-247.188042	16.764648	8.684775
-245.277675	20.478474	8.694771
-243.144266	25.282484	8.704768
-241.466214	16.291393	8.714765
-239.413677	13.526271	8.724762
-237.580333	16.200826	8.734759
-235.894005	18.115696	8.744755
-233.931823	11.130300	8.754752
-231.893547	12.955842	8.764749
-230.361649	18.039021	8.774746
-228.507202	18.411287	8.784743
-226.242468	19.967010	8.794739
-224.364665	18.207148	8.804736
-222.588599	17.084046	8.814733
-220.526403	14.876341	8.824730
-218.842848	11.499079	8.834727
-217.033895	7.342338	8.844723
-215.023516	8.839191	8.854720
-213.130499	7.615328	8.864717
-211.510411	8.403953	8.874714
-209.447800	5.833038	8.884711
-207.541936	8.608145	8.894707
-205.366995	7.934552	8.904704
-203.898656	15.189453	8.914701
-202.134101	8.584565	8.924698
-200.355698	0.692219	8.934695
-198.029124	3.895977	8.944691
-196.155317	7.577781	8.954688
-194.705871	4.296318	8.964685
-192.635890	3.246332	8.974682
-191.025831	2.415008	8.984679
-189.077804	4.379724	8.994675
-186.564597	1.582183	9.004672
-185.160007	3.758363	9.014669
-183.361038	-4.225671	9.024666
-181.345044	3.066577	9.034663
-179.469832	3.752933	9.044659
-177.696786	3.212972	9.054656
-175.687073	7.866254	9.064653
-173.730818	2.626574	9.074650
-171.967827	1.464544	9.084647
-170.177686	7.128650	9.094643
-168.284682	6.907446	9.104640
-166.464362	1.334204	9.114637
-164.445781	8.790267	9.124634
-162.716389	8.336231	9.134631
-160.488840	6.511134	9.144627
-158.709986	7.394460	9.154624
-157.105832	8.768292	9.164621
-155.313612	6.676354	9.174618
-153.089358	6.347040	9.184615
-151.314076	6.648315	9.194611
-149.445658	4.760536	9.204608
-147.769953	2.371409	9.214605
-145.604590	-3.177929	9.224602
-143.466628	-0.345071	9.234599
-142.076391	3.383939	9.244595
-140.416112	-2.531639	9.254592
-137.790683	5.517609	9.264589
-136.659984	-4.295535	9.274586
-134.433063	1.647847	9.284583
-132.556117	1.955018	9.294579
-130.696473	0.243916	9.304576
-128.996265	0.429292	9.314573
-127.163334	1.160329	9.324570
-124.893132	3.239479	9.334567
-122.910864	5.219313	9.344563
-121.240642	7.962617	9.354560
-119.428443	5.848569	9.364557
-117.702186	9.816084	9.374554
-115.880486	8.131572	9.384551
-113.523406	10.424239	9.394547
-111.797412	6.302914	9.404544
-110.015396	3.396328	9.414541
-108.331075	8.387374	9.424538
-106.430722	9.451878	9.434535
-104.386809	4.520365	9.444531
-102.557934	5.769959	9.454528
-100.857582	12.438442	9.464525
-98.519348	8.036286	9.474522
-97.223557	9.266728	9.484519
-95.256040	10.869995	9.494515
-92.995149	14.366969	9.504512
-91.252076	5.681387	9.514509
-89.279294	9.278014	9.524506
-87.316937	7.812659	9.534503
-85.702807	10.151257	9.544499
-83.773914	6.591259	9.554496
-82.338278	10.129907	9.564493
-80.305752	5.803384	9.574490
-77.896498	8.719337	9.584487
-76.180958	16.225411	9.594483
-74.544679	4.891633	9.604480
-72.621379	12.512982	9.614477
-70.684497	-0.401896	9.624474
-68.584422	0.194988	9.634471
-67.023894	4.155821	9.644467
-65.086228	3.706521	9.654464
-63.304183	5.407297	9.664461
-61.075675	3.457401	9.674458
-59.225395	6.399391	9.684455
-57.479889	10.692299	9.694451
-55.855440	7.791939	9.704448
-53.814834	6.603073	9.714445
-51.903224	2.876911	9.724442
-50.190005	10.726003	9.734439
-48.029073	8.177428	9.744435
-46.454768	2.705093	9.754432
-44.316717	5.394346	9.764429
-42.454736	3.266097	9.774426
-40.438413	-0.179920	9.784423
-38.756824	9.074742	9.794419
-36.877033	10.834155	9.804416
-34.989788	7.492416	9.814413
-33.389730	6.293318	9.824410
-31.156379	8.845804	9.834407
-29.282446	6.114083	9.844403
-27.803396	6.289020	9.854400
-25.835810	4.440777	9.864397
-23.713630	8.308889	9.874394
-21.769940	0.930289	9.884391
-19.840400	0.269164	9.894387
-18.083180	-0.089736	9.904384
-16.368923	3.164509	9.914381
-14.305424	2.666756	9.924378
-12.426273	5.926281	9.934375
-10.572008	6.328743	9.944371
-8.802111	7.867289	9.954368
-6.939910	0.013807	9.964365
-5.239209	17.875395	9.974362
-3.693319	36.541697	9.984359
-2.643292	78.098119	9.994355
-1.180960	122.514688	10.004352
0.000000	176.001975	10.009357
0.466695	207.928517	10.014362
1.507359	226.785337	10.019367
1.979204	271.809285	10.024371
2.326301	271.118587	10.029376
2.861461	298.869693	10.034381
3.048433	302.377146	10.039386
3.267829	308.374163	10.044391
3.253027	310.358928	10.049395
3.553972	302.175613	10.054400
3.321701	317.813616	10.059405
3.247528	304.063571	10.064410
3.759193	318.259849	10.069415
3.337305	327.473644	10.074419
3.570238	325.249433	10.079424
3.987180	324.430898	10.084429
3.791314	318.091429	10.089434
3.942211	330.787237	10.094439
3.659539	331.846483	10.099443
4.124833	324.132104	10.104448
3.956327	329.183331	10.109453
3.760165	329.437147	10.114458
3.963807	327.351649	10.119463
3.972706	332.753048	10.124467
3.762041	326.713980	10.129472
4.304184	321.773821	10.134477
4.068496	329.068728	10.139482
4.548329	330.052081	10.144487
4.250444	327.120908	10.149491
4.150271	334.329547	10.154496
4.385178	340.177447	10.159501
4.413279	345.979488	10.164506
4.458883	331.407642	10.169511
4.103320	334.755635	10.174515
4.455963	347.791439	10.179520
4.492738	339.222886	10.184525
4.715439	364.795722	10.189530
4.666967	356.346413	10.194535
4.610542	359.946319	10.199539
4.937568	363.868264	10.204544
4.999383	354.229685	10.209549
4.828247	362.034707	10.214554
5.159137	350.270052	10.219559
4.933400	352.318431	10.224563
4.835365	346.453778	10.229568
5.035961	342.842271	10.234573
5.134213	359.108842	10.239578
5.077869	350.296514	10.244583
5.017343	355.193331	10.249587
5.096072	356.797330	10.254592
5.021319	353.756443	10.259597
4.553634	370.903353	10.264602
5.192525	371.773028	10.269607
5.372352	381.195232	10.274611
5.349359	385.758065	10.279616
5.458895	384.928636	10.284621
5.459935	392.405012	10.289626
5.493775	377.223136	10.294631
5.629483	395.729362	10.299635
5.605580	394.296740	10.304640
5.480016	389.586065	10.309645
5.570275	397.071868	10.314650
6.032176	389.592963	10.319655
5.714626	396.787421	10.324659
5.813732	393.326131	10.329664
6.158151	402.852983	10.334669
5.930911	398.573265	10.339674
6.053666	397.379025	10.344679
5.658134	405.975228	10.349683
5.887407	395.784783	10.354688
6.108203	405.812329	10.359693
5.951686	402.525852	10.364698
6.104073	403.137238	10.369703
6.130474	410.286301	10.374707
5.894961	400.105333	10.379712
5.938815	405.390797	10.384717
6.418237	409.465066	10.389722
6.297531	408.454740	10.394727
6.337558	412.163854	10.399731
6.327173	423.433086	10.404736
6.850426	433.609528	10.409741
6.655704	431.675867	10.414746
7.034175	420.337231	10.419751
6.369007	413.463869	10.424755
6.645594	411.472380	10.429760
6.754070	407.334653	10.434765
6.651954	423.628525	10.439770
7.111175	427.589326	10.444775
6.651225	421.944798	10.449779
6.646764	436.527873	10.454784
7.022765	439.992592	10.459789
6.622914	447.753716	10.464794
6.741683	443.997540	10.469799
6.761086	431.025662	10.474803
6.866715	447.177613	10.479808
6.895767	446.624372	10.484813
6.773993	443.543658	10.489818
7.415803	451.067669	10.494823
6.927325	451.776548	10.499827
7.159441	470.464612	10.504832
7.705891	472.538074	10.509837
7.698579	487.752442	10.514842
7.303472	469.888653	10.519847
7.819212	482.852832	10.524851
7.489066	462.423999	10.529856
7.286260	478.880651	10.534861
7.262581	473.421984	10.539866
8.065418	479.084734	10.544871
7.887887	475.680166	10.549875
7.830207	481.180550	10.554880
8.108011	477.350112	10.559885
7.595133	484.298221	10.564890
7.839662	481.723627	10.569895
8.082158	482.227601	10.574899
8.063179	477.022075	10.579904
8.108595	477.483368	10.584909
7.893883	494.773000	10.589914
8.299849	479.880171	10.594919
8.084895	497.535702	10.599923
8.356241	492.428943	10.604928
8.326218	486.748930	10.609933
7.997365	501.230846	10.614938
8.324682	482.602097	10.619943
8.353985	493.958095	10.624947
8.380199	490.331788	10.629952
8.309189	487.760214	10.634957
8.101299	498.400257	10.639962
8.654852	493.404604	10.644967
8.506177	495.437557	10.649971
8.333329	498.456818	10.654976
8.810681	488.474323	10.659981
8.236520	489.950661	10.664986
8.572237	513.901956	10.669991
8.762116	511.787088	10.674995
9.039823	517.938897	10.680000
9.039876	512.162612	10.685005
8.665050	528.701953	10.690010
9.434739	509.630443	10.695015
9.226963	518.866977	10.700019
9.289398	516.893863	10.705024
9.344656	531.940600	10.710029
9.059921	515.215072	10.715034
9.317688	518.394313	10.720039
9.256713	514.138503	10.725043
9.564419	527.686268	10.730048
9.450591	511.332459	10.735053
9.344135	512.076600	10.740058
9.659002	504.942793	10.745063
9.280179	514.015793	10.750067
9.360776	517.709002	10.755072
9.512180	532.104883	10.760077
9.551856	532.661712	10.765082
9.798976	537.225663	10.770087
9.609337	532.499930	10.775091
9.543674	536.574446	10.780096
9.446757	526.552634	10.785101
9.876111	541.369398	10.790106
10.285417	525.111906	10.795111
9.661201	534.823310	10.800115
9.675451	530.888238	10.805120
9.653771	539.606240	10.810125
9.903721	528.822614	10.815130
9.908529	533.048317	10.820135
9.875634	531.719620	10.825139
10.148366	549.098727	10.830144
10.345228	548.698490	10.835149
10.306907	560.506880	10.840154
10.342728	554.614485	10.845159
10.529554	565.732521	10.850163
10.447555	557.687417	10.855168
10.528962	546.635767	10.860173
10.520184	551.781443	10.865178
10.275026	543.912185	10.870183
10.390628	562.164783	10.875187
10.461344	553.792543	10.880192
10.694464	561.135793	10.885197
10.324561	553.002571	10.890202
10.881247	555.563276	10.895207
10.955711	557.489681	10.900211
10.831581	551.827806	10.905216
11.154206	568.585534	10.910221
10.905413	571.137523	10.915226
11.233986	555.533128	10.920231
10.859372	570.511274	10.925235
11.066434	564.490634	10.930240
11.330284	560.917871	10.935245
10.857061	561.841943	10.940250
11.331908	559.356757	10.945255
11.289421	566.415958	10.950259
10.962088	563.834791	10.955264
11.033776	553.987921	10.960269
11.321854	561.639378	10.965274
11.319382	563.376202	10.970279
11.371238	570.060806	10.975283
11.617695	557.199259	10.980288
11.362194	560.081903	10.985293
11.262709	576.071170	10.990298
12.018350	572.162913	10.995303
11.658467	566.048196	11.000307
11.734959	567.360834	11.005312
11.623662	563.146152	11.010317
11.744858	576.613325	11.015322
12.437033	584.064718	11.020327
12.005478	573.470189	11.025331
11.692851	562.123403	11.030336
11.871353	571.109120	11.035341
12.036575	594.070591	11.040346
12.339396	579.386504	11.045351
11.905868	580.384672	11.050355
12.085031	584.681929	11.055360
12.590079	595.438566	11.060365
12.414140	594.528501	11.065370
12.906739	571.300029	11.070375
12.135024	577.102002	11.075379
12.192548	576.427517	11.080384
12.433498	571.913793	11.085389
11.984159	573.515311	11.090394
12.634709	591.187449	11.095399
12.586289	603.547852	11.100403
12.615590	609.993217	11.105408
12.859171	606.409482	11.110413
12.642441	615.683776	11.115418
13.077606	594.672206	11.120423
12.696170	589.254789	11.125427
12.467448	597.034428	11.130432
12.785184	602.769874	11.135437
12.730398	607.569664	11.140442
12.595242	596.487863	11.145447
12.565037	604.601702	11.150451
12.630165	608.384136	11.155456
12.660072	606.536048	11.160461
12.359807	610.870360	11.165466
13.073278	621.704161	11.170471
13.464621	631.447613	11.175475
13.538866	633.708384	11.180480
13.845631	621.657193	11.185485
13.532596	615.837763	11.190490
13.546032	606.992071	11.195495
13.490697	588.041015	11.200499
13.796677	600.532548	11.205504
13.362123	604.306370	11.210509
13.434885	595.293525	11.215514
13.517847	591.719643	11.220519
13.641310	610.357410	11.225523
13.556721	611.150109	11.230528
14.153702	627.652830	11.235533
13.744669	617.338533	11.240538
13.749706	610.156320	11.245543
13.578608	619.115826	11.250547
13.705312	620.552927	11.255552
13.988812	630.233154	11.260557
13.848353	639.474797	11.265562
14.432574	626.149297	11.270567
13.958855	638.869309	11.275571
14.102232	634.710180	11.280576
14.462138	639.240405	11.285581
14.519299	642.804917	11.290586
14.687215	628.505006	11.295591
14.307883	630.953244	11.300595
14.301209	624.307491	11.305600
14.460733	619.035594	11.310605
14.037182	635.633291	11.315610
14.518192	623.827124	11.320615
14.630615	637.070244	11.325619
14.405311	631.063346	11.330624
14.618710	625.279795	11.335629
14.483100	624.716540	11.340634
14.664001	638.675729	11.345639
14.438310	641.857994	11.350643
14.399884	637.846137	11.355648
14.710698	635.640997	11.360653
14.688151	634.610267	11.365658
14.659150	633.523794	11.370663
14.748613	643.454181	11.375667
14.968776	650.777466	11.380672
15.044899	656.338578	11.385677
15.349855	650.720190	11.390682
15.414138	653.326337	11.395687
15.044899	649.083384	11.400691
15.094762	656.331331	11.405696
15.528382	649.962275	11.410701
15.191181	659.858223	11.415706
15.441432	640.030437	11.420711
15.475068	652.199594	11.425715
15.488416	649.631882	11.430720
15.722096	645.079870	11.435725
15.725789	652.224790	11.440730
15.633406	645.159026	11.445735
15.596887	632.112307	11.450739
15.455979	638.343555	11.455744
15.648678	639.345922	11.460749
15.825066	651.542772	11.465754
16.146773	642.671543	11.470759
15.943000	648.283604	11.475763
15.876376	652.580662	11.480768
15.837388	653.107463	11.485773
15.956420	645.276255	11.490778
16.152626	643.425293	11.495783
15.859438	660.377549	11.500787
16.070568	653.119864	11.505792
16.370710	651.111971	11.510797
15.963945	654.559668	11.515802
16.201223	648.244008	11.520807
16.495873	643.496187	11.525811
16.386751	650.730065	11.530816
16.271255	645.497294	11.535821
16.251008	640.981054	11.540826
16.290172	644.773946	11.545831
16.387079	649.573210	11.550835
16.082785	666.144035	11.555840
16.322466	652.501298	11.560845
16.147015	653.303760	11.565850
16.510209	666.380750	11.570855
16.567958	677.658236	11.575859
16.830916	674.225940	11.580864
16.700072	676.268689	11.585869
16.744950	686.154175	11.590874
16.669351	672.093340	11.595879
16.476353	685.960821	11.600883
16.726089	682.894917	11.605888
16.994108	679.166915	11.610893
16.571444	679.660296	11.615898
16.937209	691.301835	11.620903
17.136317	699.804940	11.625907
17.120823	704.063894	11.630912
17.461917	712.528590	11.635917
17.468541	715.233833	11.640922
17.432554	705.066558	11.645927
17.131632	700.547758	11.650931
17.275769	702.616038	11.655936
17.703608	709.933038	11.660941
17.676940	712.686170	11.665946
17.810147	707.964079	11.670951
17.805061	692.766002	11.675955
17.679758	692.557501	11.680960
17.998681	692.826939	11.685965
17.346105	680.312112	11.690970
17.890227	681.059729	11.695975
17.637756	694.081975	11.700979
17.889668	707.388068	11.705984
17.873044	710.901286	11.710989
17.834217	714.870644	11.715994
17.794357	713.030517	11.720999
17.946732	721.053797	11.726003
17.770219	711.170713	11.731008
18.237001	716.024546	11.736013
17.714847	724.678979	11.741018
18.016766	722.442129	11.746023
17.901853	721.241617	11.751027
17.747430	720.906869	11.756032
18.155878	721.963142	11.761037
18.195185	742.748178	11.766042
18.715106	732.233587	11.771047
18.654350	747.303784	11.776051
18.396329	750.297257	11.781056
18.353064	751.155914	11.786061
18.741927	749.933396	11.791066
18.954153	741.022798	11.796071
18.713661	751.870081	11.801075
18.300468	749.066025	11.806080
18.749479	756.267704	11.811085
18.866869	753.386903	11.816090
18.915063	747.186517	11.821095
18.866424	752.501053	11.826099
18.900081	738.829593	11.831104
19.071820	747.013807	11.836109
18.697510	755.354509	11.841114
19.297657	742.513656	11.846119
18.924486	746.668819	11.851123
19.088793	746.448818	11.856128
19.056375	744.393028	11.861133
19.097749	748.527804	11.866138
19.123509	740.675151	11.871143
19.277381	755.036167	11.876147
19.079284	763.103544	11.881152
19.451951	770.445145	11.886157
19.284089	775.720356	11.891162
19.553630	762.320342	11.896167
19.367259	762.452750	11.901171
19.443133	772.082608	11.906176
19.604197	770.631486	11.911181
19.778636	773.499214	11.916186
19.636103	768.666538	11.921191
19.848538	766.814549	11.926195
19.994274	772.610615	11.931200
20.036191	774.693633	11.936205
19.846771	774.528474	11.941210
20.106224	764.123217	11.946215
20.117513	765.905180	11.951219
19.691237	771.855562	11.956224
20.103346	767.374404	11.961229
20.252260	759.751264	11.966234
20.128025	771.442638	11.971239
19.919942	768.826642	11.976243
19.825647	764.653345	11.981248
20.315369	785.155283	11.986253
20.179979	795.309301	11.991258
20.578674	797.635046	11.996263
20.747641	789.128724	12.001267
20.314533	782.073083	12.006272
20.667222	776.669391	12.011277
20.515866	779.057635	12.016282
20.540925	787.017678	12.021287
20.236924	777.318890	12.026291
20.611581	784.108230	12.031296
20.875561	800.033463	12.036301
20.468056	797.204834	12.041306
20.525040	788.751067	12.046311
20.359296	766.232860	12.051315
20.212368	777.890011	12.056320
20.439688	795.278236	12.061325
20.544996	802.102660	12.066330
20.803682	803.924019	12.071335
20.399615	799.574609	12.076339
20.716064	806.060996	12.081344
20.550565	789.316131	12.086349
20.014089	784.011680	12.091354
20.863934	799.690497	12.096359
20.840561	808.513013	12.101363
20.692296	789.008794	12.106368
20.526198	790.380647	12.111373
20.483537	775.574843	12.116378
20.484910	772.715697	12.121383
20.604033	781.960183	12.126387
20.366526	778.448410	12.131392
20.645761	781.091261	12.136397
20.565561	772.768197	12.141402
20.787880	778.067911	12.146407
20.493338	776.162739	12.151411
20.378410	779.896663	12.156416
20.345249	786.342608	12.161421
20.069611	782.835339	12.166426
20.628892	777.840256	12.171431
20.596107	800.921950	12.176435
20.740012	789.827029	12.181440
21.058191	769.111420	12.186445
20.600661	784.309598	12.191450
20.805548	782.834138	12.196455
20.700764	779.802682	12.201459
20.632277	780.774177	12.206464
20.737707	786.184003	12.211469
20.544437	783.247087	12.216474
20.814257	780.490206	12.221479
20.165237	788.377988	12.226483
20.427974	779.143909	12.231488
20.989558	784.181348	12.236493
20.709499	784.913767	12.241498
20.965052	781.649790	12.246503
20.688617	781.807602	12.251507
20.618248	767.192313	12.256512
20.819814	752.313673	12.261517
20.472211	763.200916	12.266522
20.637518	759.009868	12.271527
20.661026	752.110865	12.276531
20.257419	754.439988	12.281536
20.403322	753.838134	12.286541
20.046865	758.477139	12.291546
20.601328	765.696697	12.296551
20.621878	779.258963	12.301555
20.504596	766.893653	12.306560
20.551976	770.532299	12.311565
20.371255	775.621899	12.316570
20.735903	765.619344	12.321575
20.557858	764.197079	12.326579
20.307483	767.891101	12.331584
20.385904	766.287576	12.336589
20.752150	780.903335	12.341594
20.295556	779.935517	12.346599
20.322512	777.644742	12.351603
20.411570	786.966568	12.356608
20.642116	792.091504	12.361613
20.580566	794.842331	12.366618
20.740859	787.187398	12.371623
20.764791	783.334294	12.376627
20.432211	787.437260	12.381632
20.634553	776.298335	12.386637
20.447085	753.510003	12.391642
20.629589	760.136798	12.396647
20.684530	765.838529	12.401651
20.551534	767.449536	12.406656
20.737024	760.949694	12.411661
20.523069	767.228918	12.416666
20.870308	770.083277	12.421671
20.688405	770.818964	12.426675
20.427884	759.156195	12.431680
20.946230	758.416087	12.436685
20.313796	760.838481	12.441690
20.904982	764.043448	12.446695
20.686810	770.566205	12.451699
20.386667	773.460742	12.456704
20.733907	756.645960	12.461709
20.510662	775.773704	12.466714
20.833970	760.805460	12.471719
20.503273	766.972414	12.476723
20.808064	765.310705	12.481728
20.860848	761.990762	12.486733
20.786167	751.450356	12.491738
20.603941	739.155355	12.496743
20.251131	740.725723	12.501747
20.392090	739.009721	12.506752
20.405266	736.703803	12.511757
20.479805	753.274229	12.516762
20.865000	750.241900	12.521767
20.278676	750.403407	12.526771
20.086312	749.782965	12.531776
20.631675	752.353400	12.536781
20.495756	770.685017	12.541786
20.827014	763.337152	12.546791
20.435287	782.080968	12.551795
20.300527	772.845638	12.556800
20.748714	766.554636	12.561805
20.451955	780.299981	12.566810
20.273610	769.499334	12.571815
20.674782	770.528385	12.576819
20.998562	776.971011	12.581824
20.872969	761.218055	12.586829
20.435658	747.012196	12.591834
20.473723	741.411111	12.596839
20.392256	746.070119	12.601843
20.262639	742.561647	12.606848
20.441461	741.246471	12.611853
20.202248	756.297832	12.616858
20.535399	764.518602	12.621863
20.847303	771.745312	12.626867
20.412026	777.810676	12.631872
20.533422	775.008082	12.636877
20.539945	769.260625	12.641882
20.756734	768.190134	12.646887
20.489567	765.367513	12.651891
20.595674	762.378120	12.656896
20.699370	747.060919	12.661901
20.181500	750.439624	12.666906
20.196814	744.894208	12.671911
20.443444	777.271074	12.676915
20.367457	773.627881	12.681920
20.580643	784.161546	12.686925
20.340655	790.553746	12.691930
20.591116	782.712540	12.696935
20.614468	789.570532	12.701939
20.568394	782.393232	12.706944
20.737453	788.497831	12.711949
20.463369	791.239977	12.716954
20.528445	787.731981	12.721959
20.533607	785.275940	12.726963
20.380653	795.002238	12.731968
20.392913	778.106027	12.736973
20.237485	796.496771	12.741978
20.809483	775.920446	12.746983
20.629396	784.966646	12.751987
20.920237	787.233897	12.756992
20.861969	773.950815	12.761997
20.470746	755.058634	12.767002
20.571955	759.489018	12.772007
20.484861	757.924510	12.777011
20.420217	759.218675	12.782016
20.483839	751.767631	12.787021
20.458458	750.111276	12.792026
20.141296	751.751656	12.797031
20.353517	776.037696	12.802035
20.771793	785.568794	12.807040
21.153098	772.452151	12.812045
20.541748	768.741381	12.817050
20.343425	767.314464	12.822055
20.556599	761.887297	12.827059
20.444647	761.113677	12.832064
20.489724	760.865382	12.837069
20.508190	755.460601	12.842074
20.815416	750.109903	12.847079
20.746212	764.458411	12.852083
20.311895	765.382596	12.857088
20.552905	752.194518	12.862093
20.385450	761.767772	12.867098
20.879413	758.637666	12.872103
20.609844	754.538849	12.877107
20.465833	756.861261	12.882112
20.148946	764.230051	12.887117
20.385814	759.776846	12.892122
20.656303	749.859497	12.897127
20.726981	755.071422	12.902131
20.482073	755.397676	12.907136
21.016231	758.968928	12.912141
20.592440	761.151456	12.917146
20.822096	765.167894	12.922151
21.038640	766.926582	12.927155
20.797410	756.762831	12.932160
20.928166	763.131368	12.937165
20.609131	774.983130	12.942170
20.514579	755.220435	12.947175
20.596705	752.919286	12.952179
20.562594	743.595378	12.957184
20.710108	738.093535	12.962189
20.516456	734.506968	12.967194
20.471670	732.754359	12.972199
20.175874	740.125292	12.977203
20.428729	754.467366	12.982208
20.751293	759.062723	12.987213
20.250229	752.955462	12.992218
20.506146	756.513532	12.997223
20.519051	761.992514	13.002227
20.528578	766.443044	13.007232
20.855444	763.292279	13.012237
20.320616	757.948150	13.017242
20.564127	759.407636	13.022247
20.521012	769.871781	13.027251
20.404266	767.756896	13.032256
20.504463	768.803990	13.037261
20.242655	777.530472	13.042266
20.712454	770.450675	13.047271
20.774431	763.033793	13.052275
20.524998	770.217568	13.057280
20.639191	764.807765	13.062285
20.659174	760.791289	13.067290
20.660198	746.168575	13.072295
20.625821	742.165505	13.077299
20.426801	731.962712	13.082304
20.758493	722.727132	13.087309
20.455669	744.432512	13.092314
20.394776	738.814095	13.097319
20.353587	732.840867	13.102323
20.088034	733.720786	13.107328
20.512685	753.256896	13.112333
20.641965	765.548880	13.117338
20.667641	759.052451	13.122343
20.373546	754.012923	13.127347
20.739013	758.746521	13.132352
20.836503	746.686816	13.137357
20.228671	738.876874	13.142362
20.444266	742.072355	13.147367
20.160609	745.800066	13.152371
20.548221	753.853655	13.157376
20.702699	758.695025	13.162381
20.621106	770.920508	13.167386
20.934049	749.531593	13.172391
20.537230	741.576026	13.177395
20.529323	742.943144	13.182400
20.730572	742.064373	13.187405
20.310703	735.847183	13.192410
20.315844	739.569831	13.197415
20.387968	735.215453	13.202419
20.519663	743.849188	13.207424
20.692467	747.964578	13.212429
20.570125	738.350386	13.217434
20.567426	747.805097	13.222439
20.170009	749.362080	13.227443
20.319536	739.579941	13.232448
20.622048	746.286150	13.237453
20.747674	766.574103	13.242458
20.844615	749.201569	13.247463
20.900495	752.252211	13.252467
20.848220	745.867572	13.257472
20.807762	743.702675	13.262477
20.848154	751.783259	13.267482
20.718594	744.501019	13.272487
20.615845	733.469138	13.277491
20.349990	743.410533	13.282496
20.852856	748.914654	13.287501
20.654820	748.282501	13.292506
20.833628	738.385303	13.297511
20.468108	737.089139	13.302515
20.117212	730.845180	13.307520
20.337838	737.479289	13.312525
20.318464	747.616346	13.317530
20.544120	740.484037	13.322535
20.281708	740.292673	13.327539
20.391953	740.865063	13.332544
20.671714	742.709862	13.337549
20.525381	751.009467	13.342554
20.569765	746.894483	13.347559
20.250700	745.273932	13.352563
20.295674	751.327342	13.357568
20.125589	748.908722	13.362573
20.409580	751.717970	13.367578
20.361454	748.880917	13.372583
20.196417	754.791201	13.377587
20.228094	757.639117	13.382592
20.753993	755.286110	13.387597
20.747162	753.793958	13.392602
20.687824	753.193300	13.397607
20.500711	753.220168	13.402611
20.421523	750.739739	13.407616
20.473052	759.153663	13.412621
20.550359	755.549892	13.417626
20.876474	742.473619	13.422631
20.557872	746.295217	13.427635
20.575800	756.454716	13.432640
20.845944	753.205765	13.437645
20.434870	757.016882	13.442650
20.465263	755.663876	13.447655
20.432682	757.542725	13.452659
20.479289	754.977575	13.457664
20.440335	755.450756	13.462669
20.057159	764.929106	13.467674
20.571622	761.464560	13.472679
20.646504	757.847770	13.477683
20.105466	755.769811	13.482688
20.520807	754.995668	13.487693
20.408952	758.990090	13.492698
20.588016	754.851256	13.497703
20.244613	769.210387	13.502707
20.599783	778.481878	13.507712
20.629575	781.727505	13.512717
20.595425	779.839149	13.517722
20.838403	772.273541	13.522727
20.661269	763.325681	13.527731
20.443609	764.156960	13.532736
20.720226	752.330461	13.537741
20.386173	759.895958	13.542746
20.471048	764.492169	13.547751
20.471572	769.063987	13.552755
20.414230	754.379610	13.557760
20.533202	761.395018	13.562765
20.279356	767.888770	13.567770
20.460397	760.754106	13.572775
20.827943	762.337316	13.577779
20.831388	768.629176	13.582784
20.848154	767.029177	13.587789
20.876082	760.808363	13.592794
20.793731	752.057499	13.597799
20.649682	766.728616	13.602803
20.734410	769.088665	13.607808
20.732524	765.022057	13.612813
20.370522	774.373241	13.617818
20.714583	756.229554	13.622823
20.875922	758.051452	13.627827
20.675935	756.688671	13.632832
20.456695	747.622954	13.637837
20.185942	750.236824	13.642842
20.692386	755.235737	13.647847
20.652854	763.959087	13.652851
20.727402	760.848568	13.657856
20.648399	729.817342	13.662861
20.273462	728.040120	13.667866
20.520975	725.893951	13.672871
20.557147	744.055368	13.677875
20.417905	744.069869	13.682880
20.480604	758.911434	13.687885
20.463089	760.087693	13.692890
20.742944	763.020609	13.697895
20.626310	753.360552	13.702899
20.125921	737.629554	13.707904
20.270886	750.738274	13.712909
20.540569	780.145135	13.717914
20.626823	769.131968	13.722919
20.784606	764.049536	13.727923
20.631708	767.545079	13.732928
20.724762	742.542067	13.737933
20.411408	743.328682	13.742938
20.722835	734.069519	13.747943
20.819907	742.309796	13.752947
20.308059	748.855730	13.757952
20.803264	742.614011	13.762957
20.400888	745.535887	13.767962
20.334404	749.618479	13.772967
20.226212	750.522186	13.777971
20.215379	748.948669	13.782976
20.377043	758.881023	13.787981
20.532989	777.477553	13.792986
21.045630	770.629049	13.797991
20.757807	752.398490	13.802995
20.191155	753.484134	13.808000
20.764728	739.122565	13.813005
20.331684	755.327664	13.818010
20.543239	748.664392	13.823015
20.547230	743.067165	13.828019
20.580357	746.176630	13.833024
20.814422	743.512193	13.838029
20.492264	740.430259	13.843034
20.270423	730.390383	13.848039
20.327445	751.376039	13.853043
20.557665	748.390508	13.858048
20.748267	743.976227	13.863053
20.576101	747.167323	13.868058
20.455009	747.950082	13.873063
20.257553	750.128048	13.878067
20.219527	749.195976	13.883072
20.597004	760.312929	13.888077
20.337332	776.865724	13.893082
20.599519	778.297001	13.898087
20.735451	784.198718	13.903091
20.549799	789.385306	13.908096
20.881062	775.883968	13.913101
20.478270	767.145569	13.918106
20.645389	755.292377	13.923111
20.846670	753.136231	13.928115
20.475450	739.581389	13.933120
20.367537	749.895001	13.938125
20.361233	748.833285	13.943130
20.564173	749.078645	13.948135
20.351200	745.268068	13.953139
20.354761	746.467773	13.958144
20.881107	742.208105	13.963149
20.540989	749.130360	13.968154
20.617376	743.234571	13.973159
20.456922	755.720209	13.978163
20.643973	745.624566	13.983168
21.038488	744.450033	13.988173
20.579352	755.937761	13.993178
20.945218	749.003865	13.998183
20.693744	750.676346	14.003187
20.995063	750.585883	14.008192
20.649253	748.929268	14.013210
20.582544	754.834027	14.018227
20.616993	753.361123	14.023245
20.927498	750.456822	14.028263
20.530991	748.495823	14.033280
20.624814	739.203626	14.038298
20.413075	739.269035	14.043315
20.720898	750.235662	14.048333
20.671013	750.264244	14.053351
20.111596	760.975960	14.058368
20.678339	753.565107	14.063386
20.725286	765.031091	14.068403
20.651908	743.033885	14.073421
20.461158	762.789610	14.078439
20.614926	755.845735	14.083456
21.091408	745.433887	14.088474
20.685563	771.106862	14.093491
20.489492	758.466404	14.098509
20.828599	751.456791	14.103527
20.563355	754.126146	14.108544
20.507906	750.326991	14.113562
20.479683	765.347307	14.118579
20.985338	770.806861	14.123597
20.859941	781.038817	14.128615
20.880484	784.697614	14.133632
20.937187	787.512246	14.138650
20.908658	796.867557	14.143667
20.930359	786.511701	14.148685
20.887641	785.489963	14.153703
20.643880	798.517907	14.158720
21.148073	779.222926	14.163738
20.782927	791.042514	14.168755
21.000975	792.141245	14.173773
20.863003	789.549921	14.178791
20.795782	797.456397	14.183808
20.799454	796.027722	14.188826
20.604262	804.122135	14.193843
21.074068	814.860059	14.198861
21.275526	814.123407	14.203879
20.996642	827.650110	14.208896
21.518369	825.926449	14.213914
21.171147	827.751615	14.218931
21.645360	820.780193	14.223949
21.602313	816.577932	14.228967
21.384334	807.705076	14.233984
21.730953	795.448349	14.239002
21.282349	803.762501	14.244019
21.283237	794.293189	14.249037
21.357693	787.372174	14.254055
21.097242	784.005246	14.259072
21.703174	793.234190	14.264090
21.408083	810.474123	14.269107
21.343491	805.814418	14.274125
21.298658	803.092623	14.279143
21.191931	823.042662	14.284160
21.340122	824.549716	14.289178
21.243855	823.747296	14.294195
21.486805	823.895907	14.299213
21.585562	821.840173	14.304231
21.836222	827.472550	14.309248
21.861703	818.744894	14.314266
22.028324	822.979708	14.319283
21.830055	817.345622	14.324301
21.871538	826.056659	14.329319
21.910401	819.121643	14.334336
21.553848	800.755920	14.339354
21.381214	804.094758	14.344371
21.669583	818.795653	14.349389
21.948915	815.312735	14.354407
21.523505	836.298310	14.359424
21.559685	823.620752	14.364442
21.674870	823.646600	14.369459
21.902223	829.038883	14.374477
21.597320	821.913312	14.379495
21.527363	821.702856	14.384512
21.751190	818.950790	14.389530
21.469013	827.658398	14.394547
21.661106	828.851718	14.399565
21.806616	830.744581	14.404583
21.628016	828.410622	14.409600
22.211964	852.563663	14.414618
21.955320	869.169912	14.419635
22.308393	860.622782	14.424653
21.901290	846.512131	14.429671
21.935276	851.870772	14.434688
21.980616	858.416783	14.439706
22.166040	862.360753	14.444723
21.987850	863.081466	14.449741
22.010206	867.672777	14.454759
22.220747	862.983327	14.459776
22.112380	849.863197	14.464794
22.498075	853.188496	14.469811
22.547532	848.592382	14.474829
22.863757	846.837004	14.479847
22.479584	835.988227	14.484864
22.439924	822.975136	14.489882
22.083843	822.281794	14.494899
21.880714	821.557765	14.499917
22.259487	819.432201	14.504935
22.086041	825.226601	14.509952
22.328824	832.986912	14.514970
22.450055	838.564435	14.519987
22.273235	855.599945	14.525005
22.424955	857.892934	14.530023
22.203298	855.817516	14.535040
22.415866	849.284206	14.540058
22.162138	846.760884	14.545075
21.918485	851.040696	14.550093
22.283009	859.470572	14.555111
22.516537	860.411900	14.560128
22.967735	858.894535	14.565146
22.429625	856.924646	14.570163
22.797698	850.171482	14.575181
22.926546	850.338293	14.580199
22.372355	861.698892	14.585216
22.404382	851.636278	14.590234
22.437890	854.042500	14.595251
22.256134	858.940064	14.600269
22.253451	859.783790	14.605287
22.702090	879.307133	14.610304
23.051262	881.576497	14.615322
23.269296	877.798181	14.620339
22.964934	874.751260	14.625357
22.871112	856.755683	14.630375
22.542099	862.862768	14.635392
22.797140	863.086529	14.640410
23.226882	867.107932	14.645427
22.571375	866.463920	14.650445
23.297801	859.875385	14.655463
22.684981	853.402938	14.660480
22.946089	867.727568	14.665498
23.174175	873.237725	14.670515
22.986786	860.924548	14.675533
23.087947	860.131534	14.680551
22.882352	855.785306	14.685568
23.087372	864.368037	14.690586
23.049200	869.942683	14.695603
23.053102	879.200854	14.700621
23.269938	877.236387	14.705639
23.119391	881.435292	14.710656
23.045851	875.619271	14.715674
23.064886	880.336955	14.720691
23.364309	873.390241	14.725709
23.531869	873.753794	14.730727
22.974729	880.996792	14.735744
23.519066	871.997588	14.740762
23.319415	877.034862	14.745779
23.067990	879.601363	14.750797
23.432865	871.566713	14.755815
23.625423	884.319866	14.760832
23.282773	875.532918	14.765850
23.216252	870.115319	14.770867
23.362871	882.591087	14.775885
23.812767	879.371952	14.780903
23.589520	889.511056	14.785920
23.647981	868.820236	14.790938
23.641851	860.176246	14.795955
23.484779	852.191824	14.800973
23.424042	844.141705	14.805991
23.388430	850.741522	14.811008
23.608290	862.585834	14.816026
23.783992	856.742650	14.821043
23.493202	849.070560	14.826061
23.975984	848.743629	14.831079
23.733635	863.304281	14.836096
23.719074	855.172861	14.841114
23.651880	847.097029	14.846131
23.580059	850.935738	14.851149
23.648003	848.980867	14.856167
23.470454	859.762304	14.861184
23.686852	869.497797	14.866202
23.728882	877.381386	14.871219
23.746911	883.623458	14.876237
23.957936	876.980272	14.881255
23.684656	886.911855	14.886272
24.336123	883.564616	14.891290
24.308341	872.169767	14.896307
23.785958	865.978611	14.901325
23.985974	845.364345	14.906343
23.620436	862.672204	14.911360
23.735808	866.095678	14.916378
23.952188	875.857919	14.921395
23.862083	881.653206	14.926413
24.036681	879.936143	14.931431
23.952349	880.662336	14.936448
24.104201	883.984043	14.941466
24.190705	874.751128	14.946483
23.846213	884.689348	14.951501
24.046530	878.332581	14.956519
24.355815	887.096893	14.961536
24.066816	875.481015	14.966554
24.076352	886.010841	14.971571
24.030945	874.348247	14.976589
24.274045	873.051258	14.981607
24.243320	890.637649	14.986624
24.074467	885.790059	14.991642
24.143629	880.762938	14.996659
23.990850	884.664905	15.001677
24.119833	888.308005	15.006695
24.360075	901.149519	15.011712
24.170758	915.047400	15.016730
24.355959	914.429738	15.021747
24.139877	919.839301	15.026765
24.455609	907.802907	15.031783
24.407665	909.792702	15.036800
24.031134	913.104314	15.041818
24.262785	911.990042	15.046835
24.413128	905.337646	15.051853
24.602249	914.718878	15.056871
24.598532	914.678750	15.061888
24.680448	908.718373	15.066906
24.808861	909.547485	15.071923
24.302220	919.959894	15.076941
24.873820	913.798718	15.081959
24.492641	910.664943	15.086976
24.746753	920.882083	15.091994
25.311515	931.214847	15.097011
25.103387	922.118556	15.102029
24.685668	900.786355	15.107047
24.649829	910.181443	15.112064
24.536437	914.479822	15.117082
24.920260	905.938772	15.122099
24.802998	919.777975	15.127117
25.143761	916.406356	15.132135
24.969943	906.820120	15.137152
24.654540	921.722811	15.142170
25.002851	919.174237	15.147187
25.176931	934.182910	15.152205
25.229084	923.050545	15.157223
25.309418	906.002385	15.162240
25.262609	905.045784	15.167258
25.118495	905.624214	15.172275
24.688768	912.293212	15.177293
24.587583	900.548259	15.182311
24.945248	920.606829	15.187328
25.129229	945.133699	15.192346
25.380511	930.216398	15.197363
25.119193	931.828104	15.202381
25.540271	935.501704	15.207399
25.274166	930.880392	15.212416
25.287101	927.677461	15.217434
25.439558	934.988200	15.222451
25.115848	930.599441	15.227469
25.537426	933.514777	15.232487
25.681060	932.126684	15.237504
25.532537	924.670958	15.242522
25.641279	917.300041	15.247539
25.284599	905.241912	15.252557
25.605499	901.316625	15.257575
25.635168	899.731213	15.262592
25.497481	904.057059	15.267610
25.595229	896.178257	15.272627
25.236691	902.873647	15.277645
25.598207	897.483719	15.282663
25.877172	917.864718	15.287680
25.568979	919.387947	15.292698
25.641665	906.570789	15.297715
25.707388	925.146981	15.302733
25.877817	919.941676	15.307751
25.701755	917.431122	15.312768
25.808250	904.882274	15.317786
26.014284	908.256692	15.322803
25.058269	909.279218	15.327821
25.523647	916.939577	15.332839
25.992840	926.180193	15.337856
25.796043	929.340447	15.342874
25.871033	928.970020	15.347891
26.114785	936.499002	15.352909
26.171143	926.353806	15.357927
26.139856	928.852171	15.362944
25.780047	925.210052	15.367962
26.009362	928.865474	15.372979
25.975669	933.783491	15.377997
26.274454	927.812110	15.383015
25.576153	930.685846	15.388032
25.759549	925.448584	15.393050
26.129358	930.791443	15.398067
25.956264	932.365483	15.403085
25.829007	931.923497	15.408103
26.195803	935.700135	15.413120
26.030856	923.705789	15.418138
26.086319	933.306549	15.423155
25.832143	932.677170	15.428173
25.622364	932.212167	15.433191
26.232391	948.754205	15.438208
26.302835	962.629575	15.443226
26.347234	960.794846	15.448243
26.537718	968.115267	15.453261
26.887762	960.496632	15.458279
26.676362	948.998877	15.463296
26.242515	937.382458	15.468314
26.635692	929.388878	15.473331
26.482402	938.964737	15.478349
26.684022	922.056086	15.483367
26.518747	928.947175	15.488384
26.386572	928.598780	15.493402
26.400523	922.630361	15.498419
26.667670	951.111071	15.503437
26.643161	958.052079	15.508455
26.633325	952.568780	15.513472
26.508320	965.877588	15.518490
26.989654	950.597962	15.523507
26.939892	962.696142	15.528525
27.065190	941.275698	15.533543
26.949630	929.238864	15.538560
26.456674	936.070538	15.543578
26.561477	921.181328	15.548595
26.347140	944.785462	15.553613
26.776547	943.200780	15.558631
27.012017	946.115916	15.563648
26.906829	962.501489	15.568666
27.619842	951.748180	15.573683
27.259306	951.654854	15.578701
26.847419	936.187381	15.583719
26.719279	917.464185	15.588736
26.862586	939.867701	15.593754
27.047321	957.125656	15.598771
27.048293	957.334887	15.603789
27.282509	947.438156	15.608807
27.249304	951.615219	15.613824
27.031039	952.971527	15.618842
26.902679	943.164089	15.623859
27.088591	950.055802	15.628877
27.130177	942.675135	15.633895
27.138459	955.105391	15.638912
26.863092	943.668179	15.643930
27.259030	944.981577	15.648947
26.841441	967.578415	15.653965
26.844163	961.459191	15.658983
27.096495	951.086095	15.664000
26.851023	976.499474	15.669018
27.504653	985.836551	15.674035
27.379981	987.604218	15.679053
27.501355	983.164902	15.684071
27.906886	980.979992	15.689088
27.743092	981.946949	15.694106
27.825942	974.573841	15.699123
27.366867	980.333637	15.704141
27.651956	976.728643	15.709159
27.908666	979.341527	15.714176
27.580976	968.713298	15.719194
27.697364	969.374447	15.724211
27.701790	970.482884	15.729229
27.688788	978.378450	15.734247
27.636110	974.053413	15.739264
27.804486	982.995985	15.744282
27.926706	983.404525	15.749299
28.171296	983.538721	15.754317
27.480805	973.338009	15.759335
27.970900	971.760948	15.764352
27.798811	970.583655	15.769370
28.035772	983.502844	15.774387
27.732821	985.659163	15.779405
27.622281	986.856722	15.784423
27.809587	985.508849	15.789440
27.908252	989.729383	15.794458
28.196129	981.902006	15.799475
28.129339	984.245597	15.804493
27.780417	987.395520	15.809511
28.106423	975.742817	15.814528
27.674350	974.916872	15.819546
28.060251	975.502001	15.824563
28.047037	983.720070	15.829581
27.519150	984.620832	15.834599
27.884997	988.616282	15.839616
27.812033	1008.897814	15.844634
28.392309	1008.003206	15.849651
28.210211	1010.955069	15.854669
28.206691	1016.746038	15.859687
28.648127	1004.300982	15.864704
28.399266	1015.227614	15.869722
28.519016	1008.345673	15.874739
28.445449	1005.018097	15.879757
28.558155	1001.453175	15.884775
28.478254	1006.496562	15.889792
28.425941	1007.747756	15.894810
28.950118	1006.031550	15.899827
28.734547	1008.203822	15.904845
28.835169	1004.557458	15.909863
29.231716	1002.504537	15.914880
28.769302	996.149605	15.919898
28.485577	983.886294	15.924915
28.538210	980.610953	15.929933
28.829177	995.077236	15.934951
28.778368	997.728162	15.939968
28.780045	1004.226148	15.944986
28.650431	1002.445909	15.950003
29.110053	1001.682229	15.955021
28.702819	1003.677435	15.960039
28.834780	990.555024	15.965056
28.802403	1010.642897	15.970074
29.100143	1003.812792	15.975091
29.321866	1005.493752	15.980109
29.015812	1001.311365	15.985127
28.882999	979.856527	15.990144
28.760709	986.596071	15.995162
28.961059	999.816838	16.000179
29.006577	1002.417795	16.005197
29.083895	1004.655035	16.010215
29.399569	997.627020	16.015232
29.208380	1003.317357	16.020250
29.320250	1004.696519	16.025267
29.283610	1000.590709	16.030285
29.102613	999.421126	16.035303
29.543247	1006.586839	16.040320
29.498026	1011.805592	16.045338
29.384652	984.192482	16.050355
29.303668	987.197425	16.055373
29.061579	1003.801506	16.060391
29.197465	1000.670182	16.065408
29.339074	1006.033737	16.070426
29.532473	1006.492271	16.075443
29.656359	1005.605964	16.080461
29.321354	999.922830	16.085479
29.363318	1012.814946	16.090496
29.357857	1011.736913	16.095514
29.403406	995.900690	16.100531
29.368887	1008.199394	16.105549
29.505498	1010.101566	16.110567
29.542546	1007.144879	16.115584
29.414338	1006.912251	16.120602
29.777208	1004.392801	16.125619
29.481533	1005.327311	16.130637
29.515050	1016.303286	16.135655
30.012024	1030.063501	16.140672
30.101373	1044.724011	16.145690
29.776377	1025.100853	16.150707
30.383879	1019.750297	16.155725
29.723056	1016.074369	16.160743
30.033194	1006.401440	16.165760
29.677529	1011.178930	16.170778
30.104096	1016.364906	16.175795
30.325084	1019.161245	16.180813
29.995981	1010.664633	16.185831
30.241835	1002.759004	16.190848
30.215746	1005.962832	16.195866
29.915959	1002.090899	16.200883
30.261361	995.388475	16.205901
29.779697	1013.290753	16.210919
29.906951	1026.919601	16.215936
29.848884	1025.853104	16.220954
30.219253	1035.268426	16.225971
30.329057	1036.102087	16.230989
30.322324	1030.821181	16.236007
30.360672	1027.121823	16.241024
30.240545	1035.485959	16.246042
30.657247	1024.971765	16.251059
30.704350	1034.981335	16.256077
30.498519	1027.297171	16.261095
30.889189	1023.120054	16.266112
31.008654	1024.029250	16.271130
31.090203	1017.405079	16.276147
30.616296	994.124883	16.281165
30.353542	990.541198	16.286183
30.429276	986.596791	16.291200
30.398027	1002.522311	16.296218
30.485579	1008.871324	16.301235
30.791694	1017.557572	16.306253
30.487215	1019.566277	16.311271
30.859216	1019.154768	16.316288
30.821632	1023.835912	16.321306
30.649555	1028.765021	16.326323
30.490791	1012.297559	16.331341
30.459099	1023.990219	16.336359
31.054459	1022.327152	16.341376
30.911670	1030.698046	16.346394
30.858395	1021.144417	16.351411
30.913256	1014.496190	16.356429
30.496911	1021.704216	16.361447
30.669099	1016.294106	16.366464
30.855146	1024.216151	16.371482
31.071023	1042.115747	16.376499
31.449490	1040.491990	16.381517
31.370735	1048.701673	16.386535
31.367859	1028.994099	16.391552
31.081189	1022.409779	16.396570
30.691700	1034.291648	16.401587
30.925931	1028.058393	16.406605
30.941101	1044.766205	16.411623
31.231175	1045.879423	16.416640
31.809566	1040.506762	16.421658
31.541564	1039.966098	16.426675
31.740818	1034.010550	16.431693
31.675390	1042.869329	16.436711
31.802725	1049.021681	16.441728
31.514975	1039.167241	16.446746
31.598980	1043.534846	16.451763
31.747650	1039.429356	16.456781
31.404447	1032.674725	16.461799
31.499775	1032.146898	16.466816
31.753080	1033.799229	16.471834
31.644046	1042.520246	16.476851
31.862174	1044.749191	16.481869
31.489079	1042.823739	16.486887
31.627023	1046.386800	16.491904
31.586309	1043.549472	16.496922
31.698198	1044.903467	16.501939
32.057290	1048.116654	16.506957
31.753357	1045.617034	16.511975
31.693945	1030.648512	16.516992
31.717658	1046.672279	16.522010
31.436617	1043.818227	16.527027
31.911672	1034.398971	16.532045
31.545294	1041.913638	16.537063
31.823435	1043.944250	16.542080
32.061144	1054.514883	16.547098
32.049855	1057.362434	16.552115
32.562587	1059.522371	16.557133
31.913315	1055.493809	16.562151
32.173035	1038.844741	16.567168
31.834568	1054.337978	16.572186
32.167833	1054.997573	16.577203
32.263976	1069.174111	16.582221
32.479112	1061.226161	16.587239
32.672077	1064.800900	16.592256
32.715778	1055.444137	16.597274
32.297146	1050.170719	16.602291
32.713568	1040.089136	16.607309
32.445668	1038.164210	16.612327
32.321452	1030.652642	16.617344
32.746778	1043.862735	16.622362
32.409846	1026.376051	16.627379
32.901057	1024.361512	16.632397
32.386152	1027.632297	16.637415
32.409922	1038.666472	16.642432
32.650170	1053.974598	16.647450
32.216244	1054.707795	16.652467
32.707827	1054.580803	16.657485
32.558617	1056.737779	16.662503
32.616947	1057.095164	16.667520
32.449191	1057.925905	16.672538
32.664006	1063.951054	16.677555
32.852595	1049.635081	16.682573
32.417682	1062.897454	16.687591
33.027680	1057.461544	16.692608
32.812586	1060.129246	16.697626
32.582710	1063.123346	16.702643
33.205480	1078.798346	16.707661
33.200054	1082.571472	16.712679
33.091787	1085.223712	16.717696
33.647011	1081.860322	16.722714
33.143447	1071.621860	16.727731
33.029268	1053.805462	16.732749
33.140390	1062.453624	16.737767
33.253321	1075.718292	16.742784
33.285951	1069.649307	16.747802
33.086714	1088.750883	16.752819
33.677814	1098.466093	16.757837
33.570724	1082.168060	16.762855
33.440691	1067.528512	16.767872
33.338529	1054.800458	16.772890
33.272528	1076.789262	16.777907
33.383341	1072.419243	16.782925
33.713602	1083.764787	16.787943
33.596357	1082.854014	16.792960
33.735615	1064.813137	16.797978
33.172193	1065.571707	16.802995
33.656076	1064.856065	16.808013
33.486294	1093.276183	16.813031
33.695097	1083.891496	16.818048
33.482168	1089.406010	16.823066
33.397772	1086.542608	16.828083
33.789772	1086.494420	16.833101
33.659903	1099.807273	16.838119
33.706559	1079.843194	16.843136
33.919687	1087.200963	16.848154
33.666137	1092.957909	16.853171
33.738924	1077.541966	16.858189
33.710786	1083.848117	16.863207
33.550999	1084.864777	16.868224
33.953236	1102.410683	16.873242
33.884160	1115.570710	16.878259
34.103448	1120.953379	16.883277
34.130715	1121.782906	16.888295
33.852471	1118.362107	16.893312
34.220404	1115.546104	16.898330
34.075137	1108.048864	16.903347
34.541292	1108.449742	16.908365
34.557204	1104.414172	16.913383
34.349956	1113.581902	16.918400
34.639561	1095.800150	16.923418
34.580733	1106.918336	16.928435
34.488785	1100.782692	16.933453
34.733527	1090.896769	16.938471
34.305465	1093.769902	16.943488
34.464324	1086.493153	16.948506
34.557743	1097.443905	16.953523
34.629955	1093.934182	16.958541
34.303950	1104.023757	16.963559
34.643170	1099.346742	16.968576
34.805148	1109.415118	16.973594
34.405582	1107.122648	16.978611
34.764808	1097.882273	16.983629
35.135170	1101.197494	16.988647
34.940029	1116.542096	16.993664
35.006111	1100.251029	16.998682
34.865074	1101.055489	17.003699
35.037722	1104.765611	17.008717
34.817210	1088.661839	17.013735
34.783552	1103.332590	17.018752
35.132578	1089.931651	17.023770
35.144279	1094.729226	17.028787
35.125085	1105.875696	17.033805
34.890968	1100.577549	17.038823
34.806056	1099.719819	17.043840
35.193922	1103.489996	17.048858
34.830572	1103.950817	17.053875
34.944721	1106.787810	17.058893
35.121037	1093.906768	17.063911
34.796909	1099.923509	17.068928
35.334103	1095.688396	17.073946
34.959085	1112.600091	17.078963
35.081702	1095.252384	17.083981
35.142580	1112.593201	17.088999
35.498138	1128.532671	17.094016
35.769923	1126.718282	17.099034
35.469372	1122.759922	17.104051
35.407074	1134.231038	17.109069
35.493387	1132.653869	17.114087
35.546684	1123.473284	17.119104
35.861070	1131.905025	17.124122
35.317792	1138.913131	17.129139
35.657872	1123.128894	17.134157
35.669385	1133.115893	17.139175
35.645998	1133.450134	17.144192
36.036903	1122.809424	17.149210
35.850915	1141.449635	17.154227
36.012855	1128.281420	17.159245
36.002825	1126.768382	17.164263
35.813482	1127.195158	17.169280
36.166321	1116.602996	17.174298
36.010252	1135.277753	17.179315
36.218330	1115.961129	17.184333
36.401971	1120.183879	17.189351
36.083601	1119.924950	17.194368
36.243880	1112.951553	17.199386
35.974158	1123.585866	17.204403
36.017217	1121.334481	17.209421
36.257885	1127.434184	17.214439
36.177133	1134.985140	17.219456
36.273688	1125.247097	17.224474
35.938023	1140.157962	17.229491
36.074041	1127.028489	17.234509
36.066214	1133.213446	17.239527
35.988003	1141.821068	17.244544
36.326853	1138.937340	17.249562
36.188536	1130.715392	17.254579
35.897887	1131.369111	17.259597
36.546381	1144.875610	17.264615
36.438317	1148.443326	17.269632
36.875000	1151.821914	17.274650
36.432972	1155.002452	17.279667
36.817838	1146.159077	17.284685
36.864762	1150.312406	17.289703
36.663813	1153.608649	17.294720
36.488903	1146.879032	17.299738
37.008236	1150.098146	17.304755
36.857810	1155.316426	17.309773
36.956374	1151.118224	17.314791
36.966572	1155.741452	17.319808
37.199986	1145.858872	17.324826
36.959541	1153.820698	17.329843
37.036589	1147.889314	17.334861
36.959539	1143.701819	17.339879
37.044507	1150.293552	17.344896
37.148455	1140.389153	17.349914
37.088843	1156.372848	17.354931
37.106754	1157.892852	17.359949
37.317831	1138.940661	17.364967
36.881374	1145.938025	17.369984
37.079395	1144.314723	17.375002
37.186515	1146.770601	17.380019
37.179157	1152.244486	17.385037
37.254304	1146.742840	17.390055
37.138338	1168.412564	17.395072
37.496084	1166.331205	17.400090
37.102675	1173.088908	17.405107
37.636477	1181.362988	17.410125
37.848131	1163.989987	17.415143
37.742545	1177.288027	17.420160
37.813357	1168.545065	17.425178
38.034750	1170.746768	17.430195
38.164371	1173.444453	17.435213
37.705208	1152.308824	17.440231
37.642235	1136.599868	17.445248
37.874177	1137.532030	17.450266
37.757399	1140.813273	17.455283
37.833156	1166.266985	17.460301
38.264105	1163.626539	17.465319
38.017406	1152.860987	17.470336
37.655702	1145.911052	17.475354
37.577579	1159.288065	17.480371
37.977327	1157.327422	17.485389
38.243384	1159.295485	17.490407
38.076610	1164.758621	17.495424
38.204211	1154.576734	17.500442
38.504817	1165.505504	17.505459
38.191492	1156.369214	17.510477
38.354354	1168.782865	17.515495
37.934682	1166.284379	17.520512
38.313236	1163.331393	17.525530
38.424256	1159.879959	17.530547
38.167024	1169.975914	17.535565
38.564102	1152.445938	17.540583
38.233868	1166.476646	17.545600
38.460048	1152.843559	17.550618
38.435619	1157.208044	17.555635
38.408468	1168.149766	17.560653
38.728541	1161.846134	17.565671
38.414666	1169.481480	17.570688
38.838314	1173.002151	17.575706
39.168611	1175.732324	17.580723
39.062060	1170.873127	17.585741
39.305632	1157.864898	17.590759
39.244539	1157.700214	17.595776
39.129884	1162.667400	17.600794
38.949309	1153.480052	17.605811
39.074082	1147.583527	17.610829
39.268072	1144.715038	17.615847
38.988756	1155.163715	17.620864
39.210258	1148.620982	17.625882
39.100712	1154.430489	17.630899
38.486579	1152.290209	17.635917
38.899466	1146.366609	17.640935
39.167601	1154.997650	17.645952
38.995308	1155.333619	17.650970
38.905837	1147.893526	17.655987
38.887012	1160.932322	17.661005
39.260805	1175.006479	17.666023
39.451896	1175.304940	17.671040
39.916461	1185.499715	17.676058
39.565679	1164.447455	17.681075
39.058565	1159.553049	17.686093
39.668342	1165.532550	17.691111
39.375738	1176.494593	17.696128
39.609442	1191.928179	17.701146
39.689967	1177.053590	17.706163
39.560943	1191.528856	17.711181
39.720370	1176.043934	17.716199
39.523582	1192.647297	17.721216
39.661035	1173.670623	17.726234
39.748031	1182.096191	17.731251
39.735721	1179.134756	17.736269
40.031249	1175.691643	17.741287
39.674479	1189.459191	17.746304
39.914147	1182.369279	17.751322
40.104383	1170.476954	17.756339
40.080352	1187.726011	17.761357
39.836410	1180.132787	17.766375
39.922637	1177.463949	17.771392
39.947441	1173.445817	17.776410
40.054483	1191.962279	17.781427
40.198711	1200.732660	17.786445
40.319892	1206.411007	17.791463
40.395704	1210.938845	17.796480
40.450195	1203.629919	17.801498
40.399009	1211.750354	17.806515
40.515036	1210.523942	17.811533
40.571888	1202.089926	17.816551
40.681708	1206.590317	17.821568
40.522637	1206.508899	17.826586
40.764207	1203.895505	17.831603
40.780277	1197.170010	17.836621
40.814969	1185.527423	17.841639
40.540854	1188.091303	17.846656
40.867303	1194.204095	17.851674
40.893520	1199.081186	17.856691
40.813842	1200.097661	17.861709
40.825154	1189.545759	17.866727
40.841760	1211.436649	17.871744
40.850456	1197.490569	17.876762
40.850089	1205.860872	17.881779
40.856117	1203.314932	17.886797
41.360386	1195.050234	17.891815
40.904926	1207.523210	17.896832
40.973239	1203.795433	17.901850
41.160474	1196.452754	17.906867
41.145000	1193.378564	17.911885
41.453150	1201.469996	17.916903
40.967133	1197.707935	17.921920
41.005521	1197.631204	17.926938
40.875909	1195.830491	17.931955
40.958183	1202.830091	17.936973
41.355936	1197.775621	17.941991
41.188337	1190.996053	17.947008
41.240087	1203.779812	17.952026
41.304191	1213.786794	17.957043
41.280297	1227.148928	17.962061
41.502085	1231.214616	17.967079
41.476919	1234.242168	17.972096
41.948478	1225.268515	17.977114
41.956181	1228.767450	17.982131
41.678330	1228.404528	17.987149
41.808345	1219.474341	17.992167
42.205942	1220.792222	17.997184
41.888872	1218.543204	18.002202
42.077287	1214.318068	18.007219
41.802348	1223.031048	18.012237
42.317204	1215.897229	18.017255
41.873276	1220.703020	18.022272
41.728672	1219.544917	18.027290
42.059214	1213.330830	18.032307
41.473487	1217.177668	18.037325
41.572619	1235.420167	18.042343
41.608625	1235.274602	18.047360
41.961014	1243.779000	18.052378
42.236019	1248.142946	18.057395
42.355937	1250.832755	18.062413
42.847930	1244.009311	18.067431
42.783334	1238.113065	18.072448
42.750955	1245.937936	18.077466
43.140902	1231.875961	18.082483
42.862999	1243.850313	18.087501
42.964298	1209.764124	18.092519
42.619680	1211.239708	18.097536
42.712316	1209.897476	18.102554
42.358413	1209.501066	18.107571
42.265410	1219.669963	18.112589
42.614715	1227.945182	18.117607
43.141191	1238.770344	18.122624
42.778356	1242.095572	18.127642
43.476503	1230.694772	18.132659
42.921226	1238.670677	18.137677
42.739880	1235.549001	18.142695
42.975466	1238.330471	18.147712
42.997706	1240.650466	18.152730
42.894693	1242.686842	18.157747
43.029159	1247.859718	18.162765
43.136615	1241.229739	18.167783
42.861566	1241.523896	18.172800
42.800621	1239.904135	18.177818
43.213893	1238.321999	18.182835
42.515898	1243.050342	18.187853
42.869857	1252.860110	18.192871
42.941593	1270.922979	18.197888
43.294540	1278.587310	18.202906
43.525026	1270.706011	18.207923
43.660304	1270.969331	18.212941
43.377817	1270.268945	18.217959
43.628857	1269.256950	18.222976
43.599636	1280.880209	18.227994
44.004021	1258.433212	18.233011
43.945272	1281.689033	18.238029
44.098354	1263.562334	18.243047
44.015517	1266.908977	18.248064
43.970260	1263.590983	18.253082
43.959118	1267.442147	18.258099
43.601452	1264.158248	18.263117
43.815364	1266.674193	18.268135
43.686417	1260.182585	18.273152
43.569237	1275.101212	18.278170
44.080525	1273.383889	18.283187
43.931479	1293.665369	18.288205
43.933281	1293.844585	18.293223
44.319132	1299.480756	18.298240
44.592712	1298.653928	18.303258
44.661348	1288.308318	18.308275
44.589004	1294.149700	18.313293
44.999718	1279.283692	18.318311
44.618344	1265.322681	18.323328
44.623624	1270.041113	18.328346
44.756183	1248.677259	18.333363
44.873844	1254.790343	18.338381
44.690851	1256.612961	18.343399
44.706641	1245.407497	18.348416
44.912025	1255.942536	18.353434
44.651767	1249.759740	18.358451
44.421739	1248.048968	18.363469
44.541153	1252.731887	18.368487
44.384344	1262.704923	18.373504
44.354976	1280.681683	18.378522
44.675528	1281.030285	18.383539
44.300172	1291.060219	18.388557
44.564786	1292.779992	18.393575
44.873802	1302.025950	18.398592
44.846032	1306.545170	18.403610
45.201615	1306.545264	18.408627
44.641947	1318.710909	18.413645
45.110311	1309.688951	18.418663
45.373720	1309.559026	18.423680
44.943053	1315.103633	18.428698
45.249143	1318.973428	18.433715
45.495000	1307.426053	18.438733
45.666813	1314.873900	18.443751
45.546880	1303.306216	18.448768
45.822757	1313.715222	18.453786
45.919360	1313.723588	18.458803
45.896455	1312.099325	18.463821
45.997033	1304.858503	18.468839
46.033116	1297.239432	18.473856
45.895447	1310.091249	18.478874
46.233877	1301.750694	18.483891
46.338391	1303.261620	18.488909
45.856516	1298.100442	18.493927
45.818958	1288.021882	18.498944
45.615774	1291.005478	18.503962
45.932459	1291.087282	18.508979
45.883663	1309.070321	18.513997
45.559180	1299.646280	18.519015
46.189995	1298.318880	18.524032
45.694951	1305.755102	18.529050
46.014861	1298.498178	18.534067
46.111454	1304.652397	18.539085
46.317716	1307.729570	18.544103
46.421821	1335.610974	18.549120
46.319645	1329.017536	18.554138
46.659172	1333.731444	18.559155
46.786478	1328.913548	18.564173
46.762398	1320.484506	18.569191
46.891732	1296.651426	18.574208
46.418888	1302.328598	18.579226
46.956010	1289.688714	18.584243
46.616686	1291.710877	18.589261
46.213279	1293.958766	18.594279
46.498934	1307.948010	18.599296
46.564441	1330.548585	18.604314
46.817338	1324.277621	18.609331
46.639032	1325.125789	18.614349
46.873369	1323.679150	18.619367
47.497367	1325.333743	18.624384
46.834492	1338.127777	18.629402
47.389781	1323.713723	18.634419
47.236950	1332.559877	18.639437
47.369541	1324.639106	18.644455
47.446437	1326.303878	18.649472
47.149759	1318.888879	18.654490
47.703029	1317.347329	18.659507
47.259468	1327.701200	18.664525
47.432937	1326.512808	18.669543
47.770836	1321.436382	18.674560
47.372726	1335.272009	18.679578
47.534234	1324.003918	18.684595
47.607113	1321.945949	18.689613
47.244481	1313.909110	18.694631
47.307816	1327.538998	18.699648
47.443645	1328.200211	18.704666
48.073625	1336.735898	18.709683
47.481049	1341.110827	18.714701
47.716678	1354.875285	18.719719
47.678274	1354.661362	18.724736
47.652050	1347.027033	18.729754
47.860106	1349.842804	18.734771
47.684100	1355.787262	18.739789
47.626680	1347.597905	18.744807
48.022563	1349.085961	18.749824
47.727162	1358.127904	18.754842
48.444244	1354.864484	18.759859
48.419033	1370.220004	18.764877
48.659814	1374.955966	18.769895
48.546683	1353.077432	18.774912
48.465785	1347.352058	18.779930
48.394241	1344.620262	18.784947
48.757722	1342.478189	18.789965
48.731577	1342.082984	18.794983
48.616836	1345.941253	18.800000
48.151109	1340.826248	18.805018
48.697830	1340.629116	18.810035
48.696666	1351.433123	18.815053
48.753500	1357.746290	18.820071
49.280768	1361.275652	18.825088
48.935953	1351.988527	18.830106
49.302444	1333.025454	18.835123
48.637669	1338.874823	18.840141
48.814632	1334.848109	18.845159
49.304379	1342.500096	18.850176
49.011102	1369.166061	18.855194
49.332272	1360.011817	18.860211
49.529928	1368.778498	18.865229
49.084573	1352.411412	18.870247
49.531225	1338.296245	18.875264
49.191363	1344.801665	18.880282
49.388438	1360.579478	18.885299
49.482862	1361.440780	18.890317
49.562573	1358.843736	18.895335
49.838069	1352.676122	18.900352
49.486466	1353.671482	18.905370
49.679061	1356.617137	18.910387
49.791975	1357.667402	18.915405
49.413277	1355.571337	18.920423
49.713018	1358.040575	18.925440
49.501226	1367.926497	18.930458
50.068231	1348.041081	18.935475
49.653165	1361.805504	18.940493
49.845869	1354.778056	18.945511
50.133000	1350.601632	18.950528
49.888851	1354.331104	18.955546
49.992696	1355.634501	18.960563
49.754548	1346.593065	18.965581
49.704048	1367.156236	18.970599
50.062765	1359.974891	18.975616
50.080960	1370.878073	18.980634
50.447101	1379.427551	18.985651
50.384006	1372.477071	18.990669
50.596199	1380.066377	18.995687
50.984017	1371.714760	19.000704
50.582300	1365.250877	19.005722
50.381210	1347.883709	19.010739
50.371886	1356.335752	19.015757
50.235502	1370.913045	19.020775
50.582757	1378.647552	19.025792
50.633513	1385.586199	19.030810
50.635656	1381.570051	19.035827
50.682995	1377.744900	19.040845
50.727925	1378.796570	19.045863
50.829558	1371.189028	19.050880
50.474108	1378.009984	19.055898
50.763246	1375.700436	19.060915
50.821287	1388.769650	19.065933
51.134862	1402.166214	19.070951
51.350312	1402.369559	19.075968
51.296947	1402.747913	19.080986
51.673725	1401.317875	19.086003
51.521849	1395.219978	19.091021
51.452072	1403.297866	19.096039
51.728406	1376.246353	19.101056
51.043550	1378.167903	19.106074
51.074472	1386.954896	19.111091
51.858792	1384.849519	19.116109
51.377109	1397.760999	19.121127
51.615548	1404.827027	19.126144
51.674940	1398.681276	19.131162
51.505231	1399.982688	19.136179
51.835952	1400.891250	19.141197
51.547023	1402.567185	19.146215
51.942546	1400.940672	19.151232
51.656056	1397.694155	19.156250
51.681528	1386.534229	19.161267
51.967758	1400.897856	19.166285
52.024738	1422.933639	19.171303
52.614010	1420.829478	19.176320
52.557751	1426.819361	19.181338
52.050045	1408.031794	19.186355
52.037936	1405.988941	19.191373
52.074967	1415.330262	19.196391
52.331258	1423.554362	19.201408
52.384341	1424.516644	19.206426
52.718527	1418.951559	19.211443
52.636524	1418.574698	19.216461
52.461762	1422.625034	19.221479
52.791576	1413.875224	19.226496
52.943633	1416.935898	19.231514
52.505224	1408.421873	19.236531
52.849350	1413.548786	19.241549
52.663613	1418.285146	19.246567
52.975550	1415.775325	19.251584
52.697862	1412.678413	19.256602
52.699009	1418.755093	19.261619
53.120366	1402.517138	19.266637
52.899213	1424.125367	19.271655
52.665028	1423.786935	19.276672
52.770612	1433.493293	19.281690
53.175662	1450.546813	19.286707
53.329923	1449.042145	19.291725
53.451857	1451.146496	19.296743
53.618335	1449.526620	19.301760
53.791257	1443.048134	19.306778
53.730610	1447.100726	19.311795
53.935836	1441.955755	19.316813
53.481989	1440.884706	19.321831
53.512502	1450.291585	19.326848
53.791053	1435.830321	19.331866
53.875027	1448.849835	19.336883
53.564657	1442.538092	19.341901
53.777365	1446.902596	19.346919
54.144162	1444.662451	19.351936
53.595855	1446.916169	19.356954
53.162105	1439.922523	19.361971
53.871660	1449.332789	19.366989
53.588846	1444.190147	19.372007
54.012021	1446.048248	19.377024
54.101157	1468.415604	19.382042
54.153773	1472.538230	19.387059
54.440290	1466.854886	19.392077
54.358850	1465.623766	19.397095
54.296900	1458.161820	19.402112
54.298990	1468.940226	19.407130
54.108174	1458.071149	19.412147
54.581872	1463.090896	19.417165
54.204451	1462.717104	19.422183
54.305677	1458.181755	19.427200
54.807479	1483.162229	19.432218
54.658780	1501.675830	19.437235
54.674817	1481.513157	19.442253
54.928127	1494.261880	19.447271
55.162109	1497.053097	19.452288
54.880631	1497.239741	19.457306
54.806909	1485.540270	19.462323
55.149991	1492.257738	19.467341
55.245760	1494.765824	19.472359
55.009746	1483.702584	19.477376
54.861861	1482.589028	19.482394
55.053677	1492.858984	19.487411
55.268351	1489.342176	19.492429
55.182189	1498.943877	19.497447
55.517750	1510.927576	19.502464
55.647889	1518.997240	19.507482
55.511391	1514.117535	19.512499
55.797876	1514.617873	19.517517
55.494900	1520.395452	19.522535
55.374797	1510.296868	19.527552
55.753156	1517.524684	19.532570
55.734647	1522.725202	19.537587
55.751561	1517.176074	19.542605
55.741329	1504.930048	19.547623
55.741820	1509.548646	19.552640
55.707981	1507.318904	19.557658
55.595986	1507.008174	19.562675
55.869576	1522.141590	19.567693
56.019741	1542.790985	19.572711
56.354481	1531.495106	19.577728
56.023352	1528.422422	19.582746
55.881502	1539.008327	19.587763
56.471178	1537.545896	19.592781
56.427911	1531.205671	19.597799
56.331439	1529.448395	19.602816
56.612904	1538.783846	19.607834
56.394979	1533.420033	19.612851
56.847221	1528.040576	19.617869
56.904966	1529.299431	19.622887
56.610815	1533.965028	19.627904
56.826836	1528.412455	19.632922
56.924203	1537.085119	19.637939
57.111390	1545.789083	19.642957
57.283488	1552.829584	19.647975
57.309239	1542.474902	19.652992
57.289215	1516.859406	19.658010
56.822585	1531.461214	19.663027
57.214332	1530.673732	19.668045
57.145187	1540.242858	19.673063
57.336978	1538.291738	19.678080
57.207361	1545.057877	19.683098
56.978010	1553.324897	19.688115
57.600383	1541.570994	19.693133
57.715817	1548.623676	19.698151
57.636161	1539.780217	19.703168
57.929491	1545.859116	19.708186
57.552785	1559.104788	19.713203
57.548004	1542.278673	19.718221
57.933321	1546.330955	19.723239
57.943784	1537.067275	19.728256
57.821595	1538.708766	19.733274
57.566294	1547.050708	19.738291
58.056230	1543.428638	19.743309
58.364895	1571.647542	19.748327
58.289266	1567.739703	19.753344
58.266172	1561.492205	19.758362
58.418850	1562.394567	19.763379
58.539151	1553.490894	19.768397
58.554840	1551.023579	19.773415
58.359877	1542.747507	19.778432
58.504761	1546.875888	19.783450
58.431447	1554.175759	19.788467
58.689121	1570.134477	19.793485
58.939758	1574.680166	19.798503
58.650237	1572.324447	19.803520
59.051328	1564.746125	19.808538
58.648257	1561.521308	19.813555
58.730198	1566.589415	19.818573
58.874395	1574.211691	19.823591
58.826740	1569.613534	19.828608
58.965513	1564.606536	19.833626
58.710428	1567.713299	19.838643
58.936467	1554.344135	19.843661
59.017228	1561.201001	19.848679
58.720136	1569.088714	19.853696
59.014833	1568.195582	19.858714
59.099189	1581.867976	19.863731
59.386453	1592.237615	19.868749
59.672580	1577.351848	19.873767
59.584050	1581.951632	19.878784
59.683564	1578.791379	19.883802
59.652156	1579.007356	19.888819
59.893647	1591.282985	19.893837
59.589385	1591.636863	19.898855
59.534565	1591.763763	19.903872
60.143815	1590.098426	19.908890
59.299020	1587.791935	19.913907
59.715985	1581.917850	19.918925
59.686932	1588.376953	19.923943
59.882599	1611.218337	19.928960
60.059701	1621.718827	19.933978
59.965383	1617.920924	19.938995
60.215221	1606.512682	19.944013
60.111080	1612.691180	19.949031
59.962979	1618.027235	19.954048
60.494298	1598.318636	19.959066
60.536775	1622.713492	19.964083
60.387992	1622.949762	19.969101
60.196284	1630.586313	19.974119
60.482238	1642.943773	19.979136
60.870485	1630.307678	19.984154
60.405198	1645.308159	19.989171
60.862072	1640.288157	19.994189
60.866259	1642.984699	19.999207
60.716075	1642.890848	20.004224
60.849349	1643.766422	20.009242
61.187851	1654.994697	20.014259
61.008009	1664.273236	20.019277
61.214839	1662.845896	20.024295
61.595258	1665.751435	20.029312
61.921859	1654.545638	20.034330
61.393196	1649.059087	20.039347
61.528676	1631.877008	20.044365
61.665027	1639.127751	20.049383
61.501862	1651.342908	20.054400
61.962690	1651.375773	20.059418
61.885985	1635.603969	20.064435
61.633438	1627.497485	20.069453
61.787608	1646.994902	20.074471
61.513530	1655.568783	20.079488
61.997361	1652.632735	20.084506
62.044220	1655.674056	20.089523
62.147906	1648.647293	20.094541
62.333295	1655.181555	20.099559
62.026656	1661.580351	20.104576
62.135262	1652.005207	20.109594
61.962714	1653.908794	20.114611
62.672991	1646.354268	20.119629
62.528016	1655.533642	20.124647
62.401790	1653.475920	20.129664
62.538897	1652.224086	20.134682
62.175237	1651.815059	20.139699
62.498764	1642.815210	20.144717
62.286701	1650.628842	20.149735
62.469632	1657.208329	20.154752
62.790654	1660.590544	20.159770
62.661289	1687.814562	20.164787
63.252367	1681.820644	20.169805
62.875043	1683.715993	20.174823
62.926483	1692.079100	20.179840
62.908695	1686.374201	20.184858
62.761407	1688.020498	20.189875
62.955887	1679.555604	20.194893
63.235899	1675.171792	20.199911
63.236258	1681.217246	20.204928
63.328226	1677.229163	20.209946
63.271973	1685.655848	20.214963
63.562307	1697.520283	20.219981
63.760759	1701.433306	20.224999
63.629375	1714.547181	20.230016
63.929164	1701.048927	20.235034
63.940270	1703.073459	20.240051
63.882238	1710.517267	20.245069
64.266116	1703.287697	20.250087
64.139892	1709.808757	20.255104
64.411249	1696.466843	20.260122
64.115618	1692.313262	20.265139
64.125128	1694.303440	20.270157
64.000685	1690.767520	20.275175
63.977407	1709.324305	20.280192
64.366580	1691.620333	20.285210
64.109570	1698.853614	20.290227
64.145417	1703.862264	20.295245
64.737866	1694.574882	20.300263
64.493759	1699.426038	20.305280
64.836312	1695.946991	20.310298
64.607842	1700.406317	20.315315
64.240274	1699.778466	20.320333
64.786509	1711.455018	20.325351
64.508991	1720.326798	20.330368
65.194872	1714.191115	20.335386
64.741026	1729.004233	20.340403
64.946455	1719.896539	20.345421
65.064538	1719.265955	20.350439
64.784728	1718.119148	20.355456
65.196370	1730.148314	20.360474
65.352305	1726.127207	20.365491
65.153721	1712.286052	20.370509
65.581698	1736.357700	20.375527
65.236338	1741.320190	20.380544
65.510404	1741.046988	20.385562
65.422134	1753.833114	20.390579
65.355611	1750.838522	20.395597
65.403486	1742.529898	20.400615
65.184422	1753.586041	20.405632
65.561115	1748.664524	20.410650
65.609681	1772.420774	20.415667
65.957942	1781.147170	20.420685
65.943664	1783.614653	20.425703
66.168968	1786.093480	20.430720
66.737675	1782.130802	20.435738
66.565943	1786.468629	20.440755
66.644612	1778.106309	20.445773
66.721209	1777.788304	20.450791
66.777689	1767.480473	20.455808
66.788614	1748.931445	20.460826
66.852526	1745.757956	20.465843
66.655922	1739.950988	20.470861
66.669824	1736.513334	20.475879
66.443972	1739.455015	20.480896
66.827682	1749.660730	20.485914
66.727852	1765.243294	20.490931
66.639734	1772.891714	20.495949
66.947450	1769.468545	20.500967
66.894896	1771.061988	20.505984
67.028893	1767.171789	20.511002
67.080845	1775.988698	20.516019
66.953503	1769.481659	20.521037
67.284098	1787.809855	20.526055
67.038589	1800.909760	20.531072
67.417369	1807.550894	20.536090
67.354967	1795.858806	20.541107
67.477819	1802.722445	20.546125
67.640112	1789.073784	20.551143
67.638341	1799.571469	20.556160
67.547309	1801.823098	20.561178
67.670197	1797.596448	20.566195
67.802611	1815.728187	20.571213
68.123080	1807.702469	20.576231
68.133547	1811.922366	20.581248
68.469378	1813.737031	20.586266
68.756303	1811.161131	20.591283
68.539875	1802.270895	20.596301
68.690794	1783.781295	20.601319
68.665823	1779.147205	20.606336
68.632251	1770.374910	20.611354
68.754947	1778.703893	20.616371
68.638440	1776.628871	20.621389
68.706422	1767.289801	20.626407
68.534307	1775.882885	20.631424
68.627565	1771.172525	20.636442
68.994036	1773.168708	20.641459
68.775985	1772.870166	20.646477
69.039570	1786.035164	20.651495
69.353066	1791.032600	20.656512
68.959922	1782.530795	20.661530
68.995853	1793.547088	20.666547
68.927463	1799.511530	20.671565
69.336648	1793.206003	20.676583
68.934745	1796.748377	20.681600
69.214224	1796.871517	20.686618
69.654911	1793.120383	20.691635
69.043940	1795.786854	20.696653
69.258853	1799.301646	20.701671
69.517022	1826.806267	20.706688
69.892787	1818.403621	20.711706
69.417499	1823.980701	20.716723
69.591493	1836.758109	20.721741
69.812633	1830.838075	20.726759
69.515176	1829.432153	20.731776
69.697753	1840.242614	20.736794
70.212459	1839.631360	20.741811
70.267064	1853.014586	20.746829
70.329603	1850.698631	20.751847
70.426752	1846.227523	20.756864
70.398112	1855.737697	20.761882
70.286877	1861.614611	20.766899
70.407871	1846.769850	20.771917
70.733516	1852.987665	20.776935
70.759684	1856.720558	20.781952
70.793679	1846.142538	20.786970
70.810927	1854.806147	20.791987
70.730096	1857.542245	20.797005
71.056184	1863.090641	20.802023
71.116207	1884.209523	20.807040
71.353480	1880.832958	20.812058
71.389467	1877.048027	20.817075
71.439506	1889.991547	20.822093
71.262892	1877.188123	20.827111
70.996617	1887.400063	20.832128
71.194802	1880.698693	20.837146
71.629223	1874.186965	20.842163
71.199229	1882.262788	20.847181
71.567175	1877.128683	20.852199
71.617549	1876.074716	20.857216
71.725344	1893.494719	20.862234
71.892909	1895.167121	20.867251
71.873550	1905.332617	20.872269
72.361922	1889.442102	20.877287
72.059892	1896.182414	20.882304
72.188260	1899.601704	20.887322
72.295650	1890.653478	20.892339
72.302674	1900.091136	20.897357
72.541333	1895.842848	20.902375
72.421319	1888.036780	20.907392
72.160227	1897.753161	20.912410
72.451797	1888.150256	20.917427
72.439554	1901.024278	20.922445
72.958992	1888.352881	20.927463
72.648057	1891.412772	20.932480
72.681221	1888.227639	20.937498
72.726766	1884.677933	20.942515
72.814564	1916.454117	20.947533
73.068933	1912.934811	20.952551
73.005175	1911.875447	20.957568
73.227962	1914.508862	20.962586
73.254952	1916.996529	20.967603
73.111057	1912.259447	20.972621
73.193767	1910.044877	20.977639
73.475614	1910.270679	20.982656
73.279213	1913.952561	20.987674
73.824035	1915.562441	20.992691
73.676515	1915.090618	20.997709
73.861822	1927.904842	21.002727
73.855432	1931.911948	21.007744
73.750936	1934.932633	21.012762
74.176178	1934.982976	21.017779
73.714525	1933.369622	21.022797
74.235303	1924.807716	21.027815
74.070867	1937.698963	21.032832
73.945336	1929.664079	21.037850
74.232210	1933.315300	21.042867
74.309526	1929.462413	21.047885
74.543962	1924.259917	21.052903
74.502279	1933.908296	21.057920
74.463078	1945.926955	21.062938
74.680920	1958.508704	21.067955
74.478628	1962.526610	21.072973
74.885878	1961.632025	21.077991
75.027659	1964.356237	21.083008
74.987558	1958.115213	21.088026
75.131419	1956.461922	21.093043
74.847833	1943.832809	21.098061
75.107598	1941.954958	21.103079
75.415040	1954.921198	21.108096
75.372127	1946.807057	21.113114
75.644301	1944.526872	21.118131
75.230624	1958.522092	21.123149
75.786796	1963.798655	21.128167
75.616716	1979.105559	21.133184
75.549009	1982.803902	21.138202
75.989548	1974.402636	21.143219
76.075768	1976.684229	21.148237
76.024826	1978.282944	21.153255
75.989704	1971.857066	21.158272
76.068699	1977.725713	21.163290
76.052991	1961.508075	21.168307
75.808285	1979.501164	21.173325
76.053245	1966.941903	21.178343
76.294174	1975.208884	21.183360
76.318792	1991.105342	21.188378
76.541967	1993.157445	21.193395
76.631201	1993.326659	21.198413
76.853999	1995.951435	21.203431
77.050971	2009.497728	21.208448
76.876193	2000.032834	21.213466
77.034464	1999.852032	21.218483
76.667878	2009.947913	21.223501
76.863025	1990.689612	21.228519
76.942226	1995.021304	21.233536
76.469277	2005.602146	21.238554
77.021763	1993.169221	21.243571
76.900620	2006.690734	21.248589
77.239321	2015.229238	21.253607
77.054024	2032.739410	21.258624
77.008075	2019.413198	21.263642
77.422934	2024.171954	21.268659
77.148417	2017.419273	21.273677
77.451520	2043.098618	21.278695
78.241997	2041.712666	21.283712
78.222491	2041.060751	21.288730
78.464565	2046.373278	21.293747
78.120892	2042.596152	21.298765
78.622434	2041.128856	21.303783
78.753669	2045.119550	21.308800
78.412227	2035.509742	21.313818
78.349187	2012.508458	21.318835
78.269506	2019.628669	21.323853
78.466851	2033.838779	21.328871
78.795237	2034.707645	21.333888
78.494782	2048.852431	21.338906
78.586899	2033.615661	21.343923
78.777973	2037.703782	21.348941
78.776653	2046.292597	21.353959
78.736702	2039.821839	21.358976
78.407362	2032.727089	21.363994
79.185795	2041.011426	21.369011
78.759954	2058.702358	21.374029
79.154426	2055.111123	21.379047
79.499274	2062.928973	21.384064
79.201959	2062.500697	21.389082
79.316623	2065.844342	21.394099
79.109422	2082.194746	21.399117
79.442091	2081.483519	21.404135
79.715952	2090.151965	21.409152
79.954525	2082.375127	21.414170
80.361449	2081.998931	21.419187
80.270691	2080.143142	21.424205
80.096215	2083.704373	21.429223
80.154032	2089.777015	21.434240
79.752168	2089.530589	21.439258
80.111844	2088.377727	21.444275
80.315313	2082.274782	21.449293
80.616404	2082.804278	21.454311
80.376041	2086.844806	21.459328
80.439944	2109.453143	21.464346
80.930865	2105.693135	21.469363
80.762806	2103.210983	21.474381
80.972160	2107.817699	21.479399
80.925432	2106.707624	21.484416
81.046448	2105.335616	21.489434
81.364333	2111.085204	21.494451
80.952252	2114.048792	21.499469
81.180652	2108.197493	21.504487
81.269285	2098.242973	21.509504
81.353811	2109.228158	21.514522
81.469456	2108.634130	21.519539
81.401022	2091.350313	21.524557
81.393050	2103.886399	21.529575
81.597096	2103.045450	21.534592
81.389554	2113.775177	21.539610
81.692008	2134.320899	21.544627
81.852623	2129.372365	21.549645
81.996229	2142.835265	21.554663
82.168817	2128.331225	21.559680
82.000513	2139.710707	21.564698
81.900991	2136.411391	21.569715
81.932402	2129.751449	21.574733
82.087691	2153.724126	21.579751
82.669054	2156.446703	21.584768
82.781967	2151.409021	21.589786
82.711131	2148.802024	21.594803
82.912526	2145.847999	21.599821
82.795144	2147.531264	21.604839
82.888157	2146.885784	21.609856
82.856695	2150.856833	21.614874
82.968059	2142.032097	21.619891
82.937051	2141.634498	21.624909
83.350429	2146.213410	21.629927
83.331184	2140.257651	21.634944
82.948134	2151.969496	21.639962
83.280495	2156.643920	21.644979
83.667996	2177.128160	21.649997
83.937429	2169.213425	21.655015
83.538674	2171.599921	21.660032
83.517076	2191.287346	21.665050
83.662510	2151.694601	21.670067
83.915161	2172.887798	21.675085
83.441285	2183.608136	21.680103
84.287971	2180.518161	21.685120
84.343618	2197.239722	21.690138
84.299747	2184.440813	21.695155
84.128602	2197.666863	21.700173
84.333492	2194.326854	21.705191
84.923380	2184.146822	21.710208
84.481998	2193.465832	21.715226
84.468097	2185.547506	21.720243
84.525494	2189.804863	21.725261
84.726552	2197.178498	21.730279
84.932077	2203.916664	21.735296
85.019295	2226.773167	21.740314
85.272233	2208.284852	21.745331
85.599954	2226.132683	21.750349
85.550601	2215.504762	21.755367
85.689385	2201.936548	21.760384
85.426087	2197.782382	21.765402
85.831155	2181.846631	21.770419
85.582002	2186.925282	21.775437
85.169970	2181.208336	21.780455
85.553855	2201.046630	21.785472
86.070473	2209.896674	21.790490
85.810238	2207.234134	21.795507
85.649359	2219.622446	21.800525
85.607442	2209.993857	21.805543
86.262765	2203.712616	21.810560
85.953279	2210.663488	21.815578
85.930902	2221.718506	21.820595
86.120245	2237.032860	21.825613
86.456774	2236.632493	21.830631
86.553536	2235.216360	21.835648
86.492521	2241.031931	21.840666
86.701317	2231.779441	21.845683
86.516973	2235.561734	21.850701
86.487909	2240.803520	21.855719
86.817834	2260.222606	21.860736
86.836695	2262.765902	21.865754
86.922566	2264.360134	21.870771
86.888896	2260.634980	21.875789
86.822557	2272.063589	21.880807
87.668446	2281.253665	21.885824
87.701077	2288.692748	21.890842
87.946241	2283.216261	21.895859
87.806690	2279.231114	21.900877
88.180511	2281.211255	21.905895
88.084099	2273.194346	21.910912
88.270933	2284.953852	21.915930
88.514681	2270.586198	21.920947
88.652639	2260.726742	21.925965
88.213156	2254.882787	21.930983
88.194065	2248.693347	21.936000
88.349445	2257.820481	21.941018
88.677763	2260.057219	21.946035
88.683651	2267.537525	21.951053
88.674052	2270.271778	21.956071
88.920083	2281.884192	21.961088
88.839525	2279.282654	21.966106
88.842871	2264.857381	21.971123
88.645589	2261.251133	21.976141
88.773320	2270.566742	21.981159
88.868069	2262.391930	21.986176
89.092339	2273.857573	21.991194
89.266135	2289.428524	21.996211
89.546930	2293.754900	22.001229
89.407590	2302.940074	22.006247
89.589942	2289.603163	22.011264
89.043015	2298.127328	22.016282
89.550921	2295.667128	22.021299
89.927380	2288.749939	22.026317
89.633170	2288.487912	22.031335
89.930178	2294.010437	22.036352
90.168276	2320.099433	22.041370
90.083903	2326.957039	22.046387
90.455749	2318.446974	22.051405
90.306735	2326.341367	22.056423
90.636144	2319.571676	22.061440
90.518691	2326.258366	22.066458
90.614518	2310.318304	22.071475
90.868176	2316.514765	22.076493
90.721683	2315.681726	22.081511
90.993904	2314.604148	22.086528
90.702644	2300.056708	22.091546
90.633922	2304.053406	22.096563
90.689875	2321.542756	22.101581
90.980939	2347.112868	22.106599
91.423500	2333.274274	22.111616
90.966381	2346.778103	22.116634
90.983076	2357.510004	22.121651
91.474594	2341.865485	22.126669
91.354927	2365.398616	22.131687
91.890796	2367.194825	22.136704
92.099275	2375.608794	22.141722
92.293798	2372.047797	22.146739
92.339115	2366.401786	22.151757
92.145773	2371.537672	22.156775
92.446362	2360.602135	22.161792
92.180276	2366.785540	22.166810
92.439401	2361.022057	22.171827
92.535404	2366.896802	22.176845
92.362763	2363.974852	22.181863
92.409249	2361.463160	22.186880
92.571836	2363.359013	22.191898
92.437740	2379.312668	22.196915
92.937546	2389.144005	22.201933
92.591248	2405.233784	22.206951
93.052135	2393.074702	22.211968
92.898409	2400.744924	22.216986
93.091582	2395.552776	22.222003
93.238622	2397.698884	22.227021
93.539963	2413.841135	22.232039
93.436947	2417.049675	22.237056
93.962731	2421.871894	22.242074
94.066469	2419.709742	22.247091
94.252049	2422.342893	22.252109
93.824886	2413.750962	22.257127
93.775365	2413.186408	22.262144
93.960127	2420.739736	22.267162
93.944934	2412.321228	22.272179
94.122707	2409.610825	22.277197
94.273920	2434.876177	22.282215
94.535332	2425.653716	22.287232
94.374573	2437.844762	22.292250
94.056792	2442.613520	22.297267
94.500999	2439.788257	22.302285
94.389707	2442.042428	22.307303
95.067139	2448.942214	22.312320
95.201541	2456.748218	22.317338
95.355390	2463.300462	22.322355
95.328841	2461.049746	22.327373
95.619885	2458.453416	22.332391
96.007473	2445.741214	22.337408
95.761606	2442.131656	22.342426
95.739727	2421.765283	22.347443
95.836753	2434.680558	22.352461
95.690869	2436.596509	22.357479
95.760991	2439.982741	22.362496
95.990167	2437.898905	22.367514
95.919210	2455.092449	22.372531
95.821827	2459.576720	22.377549
96.082020	2458.338228	22.382567
95.993879	2461.086615	22.387584
96.050048	2462.306474	22.392602
95.898534	2477.659707	22.397619
96.727386	2475.951398	22.402637
96.658448	2496.217843	22.407655
96.992217	2476.733071	22.412672
97.116096	2483.310554	22.417690
97.032448	2485.383342	22.422707
97.097475	2482.995312	22.427725
97.026384	2478.310146	22.432743
97.130692	2486.327050	22.437760
97.115231	2489.355674	22.442778
97.200791	2503.698913	22.447795
97.402309	2507.951472	22.452813
97.132051	2511.853725	22.457831
97.514854	2513.758529	22.462848
97.781336	2515.264206	22.467866
97.654717	2539.509798	22.472883
98.116866	2535.278389	22.477901
98.187176	2534.701013	22.482919
98.328968	2534.993212	22.487936
98.377329	2528.418483	22.492954
98.546628	2526.287549	22.497971
98.768946	2517.429161	22.502989
98.408452	2535.379257	22.508007
98.444820	2526.119469	22.513024
98.683968	2519.975257	22.518042
98.629611	2550.042650	22.523059
98.897993	2544.991839	22.528077
98.638574	2561.908008	22.533095
99.119221	2552.962781	22.538112
99.321338	2551.405537	22.543130
99.201860	2546.428377	22.548147
99.627709	2556.724696	22.553165
99.512387	2573.665095	22.558183
99.945299	2575.713728	22.563200
99.777946	2565.990851	22.568218
99.499373	2576.350749	22.573235
100.048897	2569.775527	22.578253
100.262254	2570.817731	22.583271
100.213458	2581.417869	22.588288
100.385328	2569.263042	22.593306
100.045282	2573.397470	22.598323
100.230122	2559.991483	22.603341
100.382822	2569.521186	22.608359
100.557180	2574.451415	22.613376
100.985898	2579.179046	22.618394
100.964020	2589.476780	22.623411
100.893059	2588.270636	22.628429
100.911520	2588.969505	22.633447
101.101056	2589.305221	22.638464
101.071892	2592.240874	22.643482
100.973875	2595.226838	22.648499
101.001777	2595.114803	22.653517
101.170059	2595.759104	22.658535
101.420969	2618.415495	22.663552
101.592651	2615.134962	22.668570
101.296197	2619.460673	22.673587
101.581964	2608.932408	22.678605
101.637434	2634.522504	22.683623
102.135551	2639.605638	22.688640
102.273300	2637.442750	22.693658
101.998351	2644.758801	22.698675
102.785342	2637.836551	22.703693
102.200074	2638.127494	22.708711
102.467090	2646.197984	22.713728
102.646618	2642.072182	22.718746
102.678894	2643.921993	22.723763
103.106451	2663.914421	22.728781
103.028881	2667.813518	22.733799
103.162686	2666.721806	22.738816
103.109732	2667.672765	22.743834
103.039730	2662.558673	22.748851
103.548083	2665.635164	22.753869
103.347763	2661.691851	22.758887
103.832781	2660.870568	22.763904
103.598671	2662.733757	22.768922
103.459204	2681.903400	22.773939
103.808319	2684.581314	22.778957
104.172230	2689.378310	22.783975
104.126240	2685.910654	22.788992
104.257409	2685.133998	22.794010
104.084373	2696.280262	22.799027
104.331636	2686.443205	22.804045
104.580707	2692.266928	22.809063
104.669464	2699.320492	22.814080
104.850142	2708.178007	22.819098
105.134355	2715.964981	22.824115
105.048847	2706.126702	22.829133
105.081326	2710.122317	22.834151
105.403434	2709.562988	22.839168
105.673246	2701.140555	22.844186
105.635496	2701.136526	22.849203
105.515893	2709.834266	22.854221
105.179874	2706.620516	22.859239
105.067863	2711.177203	22.864256
105.139760	2702.066596	22.869274
105.190115	2715.780877	22.874291
105.689054	2728.227225	22.879309
105.620533	2736.814578	22.884327
105.740132	2740.075787	22.889344
105.996755	2746.730545	22.894362
106.272296	2761.525926	22.899379
106.231095	2756.935015	22.904397
106.472034	2762.819058	22.909415
106.530765	2768.750251	22.914432
106.739878	2757.836872	22.919450
106.558373	2763.409141	22.924467
106.934718	2780.047981	22.929485
106.900996	2786.207092	22.934503
107.074350	2780.402849	22.939520
107.656761	2780.478484	22.944538
107.401413	2785.068277	22.949555
107.591824	2787.771519	22.954573
107.667285	2780.623644	22.959591
107.402808	2785.549197	22.964608
107.814461	2803.900365	22.969626
107.670570	2812.591813	22.974643
108.199432	2800.570223	22.979661
108.590258	2813.676537	22.984679
108.724638	2806.815016	22.989696
108.883869	2800.330249	22.994714
108.409086	2812.291653	22.999731
108.458030	2817.104308	23.004749
109.049763	2800.611886	23.009767
108.867829	2808.056346	23.014784
109.267344	2799.412591	23.019802
108.836636	2809.612062	23.024819
109.017035	2805.405843	23.029837
108.817527	2812.487339	23.034855
108.811841	2832.599429	23.039872
109.173481	2831.043463	23.044890
109.473381	2829.797824	23.049907
109.368204	2836.261753	23.054925
109.366987	2849.602882	23.059943
109.348058	2849.296943	23.064960
109.891830	2858.858866	23.069978
109.893754	2877.255799	23.074995
110.142164	2868.150765	23.080013
110.139375	2859.337507	23.085031
110.078354	2881.093834	23.090048
110.660926	2880.946050	23.095066
110.316433	2878.282660	23.100083
110.421460	2881.547012	23.105101
110.722625	2880.842350	23.110119
110.597392	2891.930010	23.115136
111.217254	2899.079898	23.120154
111.062286	2902.467521	23.125171
111.600672	2907.932127	23.130189
110.956627	2908.888473	23.135207
111.203040	2906.492688	23.140224
111.899200	2902.325333	23.145242
111.748357	2900.687469	23.150259
111.566264	2905.912206	23.155277
111.892250	2906.862535	23.160295
111.668695	2901.299309	23.165312
112.089449	2915.695694	23.170330
112.249822	2929.570404	23.175347
112.186676	2925.101717	23.180365
112.548097	2922.664779	23.185383
112.210214	2924.701869	23.190400
112.470533	2914.735148	23.195418
112.609320	2931.871421	23.200435
112.789726	2938.705183	23.205453
112.723983	2946.758897	23.210471
112.934438	2960.817583	23.215488
113.195854	2947.963028	23.220506
113.174696	2952.258307	23.225523
113.022910	2956.955136	23.230541
113.354254	2973.102664	23.235559
113.471661	2974.788700	23.240576
114.189574	2960.990563	23.245594
113.555358	2981.385579	23.250611
113.752660	2976.115480	23.255629
114.202999	2976.369501	23.260647
113.883718	3012.783973	23.265664
114.337437	3003.008962	23.270682
114.161538	3004.978542	23.275699
114.333999	3016.490791	23.280717
114.527706	3008.081892	23.285735
114.263280	3022.723727	23.290752
114.801733	3029.336035	23.295770
115.044213	3032.908878	23.300787
115.243470	3034.495341	23.305805
115.401237	3037.602648	23.310823
115.259224	3032.393717	23.315840
115.538895	3029.921028	23.320858
115.288449	3044.234211	23.325875
115.510421	3051.891274	23.330893
116.316423	3055.546531	23.335911
115.765040	3058.386991	23.340928
116.179979	3061.985044	23.345946
116.618037	3056.320977	23.350963
116.568934	3057.563966	23.355981
116.442160	3059.936332	23.360999
116.295565	3057.987060	23.366016
116.615448	3053.480067	23.371034
116.597118	3053.490246	23.376051
116.800427	3047.713372	23.381069
117.168724	3059.415466	23.386087
116.917292	3073.992351	23.391104
117.077279	3071.285450	23.396122
117.661857	3068.145856	23.401139
117.541071	3068.804023	23.406157
117.580361	3077.208408	23.411175
117.462792	3068.086096	23.416192
117.367383	3064.649042	23.421210
117.848679	3063.410643	23.426227
117.462479	3076.062939	23.431245
118.005473	3101.579259	23.436263
117.686981	3109.793718	23.441280
118.118304	3106.979828	23.446298
118.268071	3105.036781	23.451315
117.884120	3113.053227	23.456333
118.319891	3124.357598	23.461351
118.508186	3131.518998	23.466368
118.564092	3117.201708	23.471386
118.886407	3128.648460	23.476403
118.899392	3143.782651	23.481421
119.522131	3138.045840	23.486439
119.183278	3158.701568	23.491456
119.395859	3157.285759	23.496474
119.343693	3154.578849	23.501491
119.697133	3150.768925	23.506509
119.763619	3147.413015	23.511527
119.749236	3148.803866	23.516544
120.058141	3167.076697	23.521562
119.911717	3178.359887	23.526579
120.014662	3179.882276	23.531597
120.359399	3167.177074	23.536615
120.008657	3187.439856	23.541632
120.612815	3197.594927	23.546650
120.774923	3201.495277	23.551667
121.116114	3205.208174	23.556685
121.010967	3201.797812	23.561703
121.080796	3209.327400	23.566720
121.478655	3200.795376	23.571738
121.453171	3206.737816	23.576755
121.138737	3211.244341	23.581773
121.553743	3209.859964	23.586791
121.409467	3220.338918	23.591808
121.910746	3233.015809	23.596826
121.801947	3224.095736	23.601843
121.739162	3226.433538	23.606861
122.331729	3238.212501	23.611879
122.243941	3246.534200	23.616896
122.699490	3252.432991	23.621914
122.462920	3254.292711	23.626931
122.672325	3249.108688	23.631949
123.118280	3242.553620	23.636967
122.736031	3246.742161	23.641984
122.879177	3242.570076	23.647002
122.955587	3245.039864	23.652019
123.220134	3256.915985	23.657037
123.596499	3253.967666	23.662055
123.136440	3269.305639	23.667072
123.871057	3251.134874	23.672090
123.993061	3261.821542	23.677107
123.577524	3258.776097	23.682125
124.056586	3258.504014	23.687143
124.052428	3259.124714	23.692160
123.956649	3277.098006	23.697178
124.450260	3284.230463	23.702195
124.238824	3276.222690	23.707213
124.502950	3281.379552	23.712231
124.659536	3276.477687	23.717248
124.635973	3281.962036	23.722266
124.899833	3280.162032	23.727283
125.318233	3303.098779	23.732301
125.382814	3290.364988	23.737319
125.357765	3309.142772	23.742336
125.305667	3307.555191	23.747354
125.303977	3309.346000	23.752371
125.235457	3305.648160	23.757389
125.624196	3313.406202	23.762407
125.200343	3325.407096	23.767424
125.856285	3333.209857	23.772442
125.775030	3340.218472	23.777459
125.481403	3357.354974	23.782477
126.077833	3352.264166	23.787495
126.164882	3369.291209	23.792512
126.265928	3367.562781	23.797530
127.054237	3377.268555	23.802547
127.266802	3395.527143	23.807565
127.110423	3380.164975	23.812583
127.493915	3388.520947	23.817600
127.573514	3387.389056	23.822618
127.542562	3386.889152	23.827635
127.415056	3387.900815	23.832653
127.741278	3379.963791	23.837671
127.750871	3380.609048	23.842688
127.997941	3401.804139	23.847706
128.239181	3404.839218	23.852723
127.842769	3413.287313	23.857741
128.487047	3406.880688	23.862759
128.130244	3417.890823	23.867776
128.550514	3419.606494	23.872794
128.832637	3407.324051	23.877811
128.766524	3423.289242	23.882829
129.152965	3434.545871	23.887847
129.174145	3434.813272	23.892864
129.146459	3437.953384	23.897882
129.558141	3441.643303	23.902899
129.161250	3442.222012	23.907917
129.882145	3442.438411	23.912935
129.470879	3447.618072	23.917952
129.834659	3449.040687	23.922970
129.917100	3465.691780	23.927987
130.089361	3459.135422	23.933005
130.417597	3459.199682	23.938023
130.348612	3463.564094	23.943040
130.305582	3456.824169	23.948058
130.115080	3455.119408	23.953075
130.342119	3479.677521	23.958093
130.702455	3474.052435	23.963111
130.559840	3494.269866	23.968128
130.648620	3492.727452	23.973146
131.103225	3498.875074	23.978163
131.128343	3514.034459	23.983181
131.475976	3520.297477	23.988199
131.413558	3515.938622	23.993216
131.267435	3515.702509	23.998234
131.867687	3533.082133	24.003251
131.799170	3542.871154	24.008269
131.935677	3554.908744	24.013287
131.805697	3548.618439	24.018304
132.039017	3551.394434	24.023322
132.130272	3548.557598	24.028339
132.448327	3581.234434	24.033357
132.764007	3570.884001	24.038375
133.172741	3568.013057	24.043392
132.996184	3561.125248	24.048410
133.203593	3557.764080	24.053427
133.250827	3567.636923	24.058445
133.787551	3579.440802	24.063463
133.892008	3583.598240	24.068480
133.888796	3592.601253	24.073498
134.172498	3580.399439	24.078515
134.301104	3574.960727	24.083533
134.498014	3574.012283	24.088551
134.638945	3578.122998	24.093568
134.708324	3578.985284	24.098586
134.671879	3579.444378	24.103603
134.484449	3575.529438	24.108621
134.899239	3569.626602	24.113639
134.891479	3575.704815	24.118656
134.616666	3570.440562	24.123674
134.931189	3575.348782	24.128691
135.263676	3592.304697	24.133709
135.662478	3595.906247	24.138727
135.639303	3593.436918	24.143744
135.738931	3602.457364	24.148762
135.768588	3594.790920	24.153779
135.599660	3609.467669	24.158797
135.975469	3607.416143	24.163815
135.975499	3625.004863	24.168832
135.654707	3635.412355	24.173850
136.187813	3637.988742	24.178867
136.362914	3641.865114	24.183885
136.573979	3645.242525	24.188903
136.696469	3652.756080	24.193920
136.890310	3652.782774	24.198938
137.488822	3664.248839	24.203955
137.313771	3675.929512	24.208973
137.714017	3674.897507	24.213991
137.758841	3671.246793	24.219008
137.794859	3668.666536	24.224026
138.078923	3666.971035	24.229043
138.001849	3672.541941	24.234061
137.918291	3667.076454	24.239079
138.062626	3672.171534	24.244096
138.092660	3671.296105	24.249114
138.140785	3684.730031	24.254131
138.091085	3694.226667	24.259149
138.099254	3699.484278	24.264167
138.464462	3712.277684	24.269184
138.663842	3728.457320	24.274202
139.495287	3723.228224	24.279219
139.404035	3719.603129	24.284237
139.736677	3716.708892	24.289255
139.825581	3716.214251	24.294272
139.690266	3697.135411	24.299290
140.144715	3693.749768	24.304307
139.536035	3710.853532	24.309325
140.278522	3723.844025	24.314343
140.560041	3733.375977	24.319360
140.065503	3740.738595	24.324378
140.486795	3737.281924	24.329395
140.573251	3740.498298	24.334413
140.743251	3742.295609	24.339431
140.693035	3751.346333	24.344448
140.595000	3767.813365	24.349466
141.128463	3760.061782	24.354483
141.221875	3784.643288	24.359501
141.429568	3775.962687	24.364519
141.795198	3770.951807	24.369536
141.813365	3794.193074	24.374554
142.086566	3783.201065	24.379571
141.954683	3795.730040	24.384589
141.994206	3791.523192	24.389607
142.188118	3800.043362	24.394624
142.254859	3806.134963	24.399642
142.571732	3816.099498	24.404659
142.624977	3820.553085	24.409677
143.167678	3820.904894	24.414695
143.308568	3834.909437	24.419712
143.123112	3843.937730	24.424730
143.351723	3836.698843	24.429747
143.366987	3836.116821	24.434765
143.802216	3839.782638	24.439783
143.376994	3836.590719	24.444800
143.532425	3860.469421	24.449818
143.891923	3870.892897	24.454835
143.810629	3865.672412	24.459853
144.150094	3867.183907	24.464871
144.646394	3886.309602	24.469888
144.607398	3896.765170	24.474906
144.707298	3886.979130	24.479923
144.917374	3894.328592	24.484941
144.867716	3896.396157	24.489959
145.134519	3911.059582	24.494976
145.210055	3925.916358	24.499994
145.371330	3915.174162	24.505011
145.364567	3922.195563	24.510029
145.369087	3931.755292	24.515047
145.863952	3915.022199	24.520064
145.923781	3942.634028	24.525082
146.540054	3940.752582	24.530099
146.730668	3940.781366	24.535117
146.516870	3943.657836	24.540135
146.902281	3941.830507	24.545152
146.992129	3931.322313	24.550170
147.310643	3938.818133	24.555187
146.868883	3931.215667	24.560205
147.163584	3937.975822	24.565223
147.138176	3925.387988	24.570240
146.962901	3947.206595	24.575258
147.545027	3954.119954	24.580275
147.254330	3960.609237	24.585293
147.501605	3957.009558	24.590311
147.396950	3979.818372	24.595328
147.488138	3996.732206	24.600346
148.140080	3981.314466	24.605363
148.249371	4018.661370	24.610381
148.496006	4008.670133	24.615399
148.831531	4019.849589	24.620416
148.920414	4016.943029	24.625434
148.931140	4019.554795	24.630451
149.513557	4029.721002	24.635469
149.332218	4037.406706	24.640487
149.411107	4038.597902	24.645504
149.541174	4043.239908	24.650522
149.641637	4038.741645	24.655539
149.682631	4048.261808	24.660557
149.917614	4065.746727	24.665575
150.304488	4056.809257	24.670592
150.086017	4063.076242	24.675610
150.561470	4069.645585	24.680627
150.877798	4084.147888	24.685645
150.933900	4076.915150	24.690663
151.360475	4081.459543	24.695680
151.132785	4089.420918	24.700698
151.313476	4081.176324	24.705715
151.364263	4084.451168	24.710733
151.487136	4081.587949	24.715751
151.871218	4101.431168	24.720768
151.695090	4108.579569	24.725786
151.955147	4102.806610	24.730803
151.943617	4117.051274	24.735821
152.507958	4117.809498	24.740839
152.565447	4136.700262	24.745856
152.752632	4129.666078	24.750874
152.770800	4121.001333	24.755891
152.681064	4137.154361	24.760909
152.826990	4132.500140	24.765927
153.480251	4140.893774	24.770944
153.239541	4156.303891	24.775962
153.600933	4157.763148	24.780979
153.710950	4157.202194	24.785997
154.054398	4162.533165	24.791015
153.737855	4161.528100	24.796032
153.842777	4167.458790	24.801050
154.320646	4167.935017	24.806067
154.150089	4188.728195	24.811085
154.282075	4190.470263	24.816103
154.792733	4176.856664	24.821120
154.229829	4190.772377	24.826138
154.625437	4201.755165	24.831155
154.896957	4214.211521	24.836173
155.279082	4214.946099	24.841191
155.772097	4215.797516	24.846208
155.661817	4232.392888	24.851226
155.661135	4226.519067	24.856243
155.708263	4229.203733	24.861261
155.814002	4233.898452	24.866279
156.023550	4235.941256	24.871296
156.342962	4248.246044	24.876314
156.481472	4258.516231	24.881331
156.663442	4259.389713	24.886349
156.556445	4263.647928	24.891367
157.212046	4268.524816	24.896384
157.025805	4287.304379	24.901402
157.318812	4281.939103	24.906419
157.396776	4288.221852	24.911437
157.709104	4283.037578	24.916455
158.219838	4304.921191	24.921472
158.234139	4303.344942	24.926490
158.369464	4296.352775	24.931507
158.800997	4313.059306	24.936525
158.731133	4299.096042	24.941543
159.057066	4299.077291	24.946560
158.918487	4304.545747	24.951578
158.969896	4297.064271	24.956595
159.287100	4297.998794	24.961613
159.162572	4300.587335	24.966631
159.117967	4301.127207	24.971648
159.092625	4315.434052	24.976666
159.266285	4317.859410	24.981683
159.885462	4320.262507	24.986701
160.017454	4344.096173	24.991719
160.644989	4338.749913	24.996736
160.305085	4358.388737	25.001754
160.750937	4342.363911	25.006771
161.246139	4343.614623	25.011789
160.808758	4345.258689	25.016807
160.996725	4335.828836	25.021824
161.233829	4346.451533	25.026842
161.068536	4353.119235	25.031859
161.305224	4360.690468	25.036877
161.394746	4361.736033	25.041895
161.481896	4365.149105	25.046912
161.786343	4394.012155	25.051930
162.191051	4390.015956	25.056947
162.226767	4398.948748	25.061965
161.919865	4406.623983	25.066983
162.046912	4397.451611	25.072000
162.125466	4417.571325	25.077018
162.438958	4414.323641	25.082035
162.908565	4428.591015	25.087053
162.903329	4435.753235	25.092071
163.713465	4438.498009	25.097088
163.441007	4444.300177	25.102106
163.630491	4450.986879	25.107123
164.111028	4445.018936	25.112141
163.990981	4448.175563	25.117159
164.066539	4444.607079	25.122176
163.941691	4457.492651	25.127194
164.484263	4466.766335	25.132211
164.519796	4462.476542	25.137229
164.408884	4476.338549	25.142247
164.692474	4481.584781	25.147264
164.730273	4504.545554	25.152282
165.113943	4504.208429	25.157299
165.390831	4506.111518	25.162317
165.374774	4513.712901	25.167335
165.811371	4517.873504	25.172352
166.198120	4521.467772	25.177370
166.117693	4513.685450	25.182387
166.160075	4523.566004	25.187405
166.304408	4531.165424	25.192423
166.798492	4536.598388	25.197440
166.884471	4540.562373	25.202458
166.622582	4552.433017	25.207475
167.097256	4543.092631	25.212493
167.159852	4560.394007	25.217511
167.397198	4559.620783	25.222528
167.468066	4568.071337	25.227546
167.631633	4563.713899	25.232563
167.497500	4580.843699	25.237581
168.048770	4596.598444	25.242599
167.765550	4599.055786	25.247616
168.364899	4609.469871	25.252634
168.635337	4624.838313	25.257651
169.016697	4628.019664	25.262669
168.976562	4635.281162	25.267687
169.205246	4624.316868	25.272704
169.110321	4623.768905	25.277722
169.201132	4636.371652	25.282739
169.257275	4649.950723	25.287757
169.253895	4654.301094	25.292775
169.765358	4667.784771	25.297792
170.086994	4671.862265	25.302810
170.291293	4679.438040	25.307827
170.664898	4683.330243	25.312845
170.310559	4675.705579	25.317863
170.857111	4697.399982	25.322880
171.118393	4699.646226	25.327898
171.170447	4713.286584	25.332915
171.406142	4692.932627	25.337933
171.407015	4701.883746	25.342951
171.870724	4700.591390	25.347968
171.977513	4693.896238	25.352986
171.611209	4700.714151	25.358003
172.214723	4701.161715	25.363021
172.146575	4716.499274	25.368039
172.384764	4716.917761	25.373056
172.445919	4722.906004	25.378074
172.468481	4718.634725	25.383091
172.748031	4739.848605	25.388109
172.798640	4753.223324	25.393127
172.749851	4757.639968	25.398144
173.115841	4768.170045	25.403162
173.102894	4785.788185	25.408179
173.600355	4776.323654	25.413197
173.800463	4789.030259	25.418215
173.839071	4805.860577	25.423232
173.982642	4814.627739	25.428250
174.244670	4799.796841	25.433267
174.848318	4823.383010	25.438285
174.652709	4814.587519	25.443303
175.111008	4822.736503	25.448320
175.290374	4816.548165	25.453338
175.155045	4825.659535	25.458355
175.394770	4832.350989	25.463373
175.847621	4843.847510	25.468391
175.805709	4846.434774	25.473408
176.060979	4839.394119	25.478426
176.037013	4858.977727	25.483443
176.333368	4862.105814	25.488461
176.208650	4868.640619	25.493479
176.733350	4870.701711	25.498496
177.164840	4877.748886	25.503514
177.061136	4900.311948	25.508531
177.213428	4906.918250	25.513549
177.793475	4896.319413	25.518567
177.901189	4900.505029	25.523584
177.765218	4889.718258	25.528602
178.243075	4901.391781	25.533619
178.408297	4915.413933	25.538637
178.271330	4917.182449	25.543655
178.110903	4921.355753	25.548672
178.613512	4922.532176	25.553690
178.561458	4942.939342	25.558707
179.131649	4950.965139	25.563725
179.229007	4946.294019	25.568743
179.100872	4946.953438	25.573760
179.387538	4958.635461	25.578778
179.570347	4975.471305	25.583795
179.998148	4975.846983	25.588813
179.890624	4985.784004	25.593831
179.963791	4998.127898	25.598848
180.234421	4996.057558	25.603866
180.349037	5004.517909	25.608883
180.444795	5017.002186	25.613901
180.620031	5026.902807	25.618919
181.096793	5041.479608	25.623936
181.230067	5035.174225	25.628954
181.416543	5050.140326	25.633971
181.963407	5046.885194	25.638989
181.913718	5073.526916	25.644007
181.760536	5070.398339	25.649024
182.017915	5066.317671	25.654042
181.889755	5058.418369	25.659059
182.121860	5077.900864	25.664077
182.493356	5083.812239	25.669095
182.709660	5090.413926	25.674112
182.915078	5091.412744	25.679130
183.272889	5111.926303	25.684148
183.550407	5111.704435	25.689165
183.605214	5119.954106	25.694183
183.734717	5120.594484	25.699200
184.220844	5132.045017	25.704218
184.047813	5138.120329	25.709236
184.431843	5142.234426	25.714253
184.485203	5145.310842	25.719271
184.645338	5169.507974	25.724288
184.924349	5168.257616	25.729306
184.785149	5173.399213	25.734324
184.957681	5166.538381	25.739341
185.331051	5192.946083	25.744359
185.353874	5194.419308	25.749376
185.541860	5194.832441	25.754394
185.935347	5214.084051	25.759412
186.289701	5216.524809	25.764429
186.345866	5222.717813	25.769447
186.648849	5230.570017	25.774464
186.995027	5236.808050	25.779482
187.142322	5232.591476	25.784500
187.400466	5233.504012	25.789517
187.333339	5243.600765	25.794535
187.377540	5233.552865	25.799552
187.588984	5243.845944	25.804570
187.719335	5254.254235	25.809588
187.952577	5268.348485	25.814605
187.742058	5272.293854	25.819623
187.994131	5287.317396	25.824640
188.544180	5290.324883	25.829658
188.432558	5304.005257	25.834676
189.234990	5310.069878	25.839693
189.020876	5321.913853	25.844711
189.193618	5323.336440	25.849728
189.855274	5337.702323	25.854746
189.891181	5346.357943	25.859764
190.295056	5338.843347	25.864781
190.208041	5349.610495	25.869799
190.117874	5349.195490	25.874816
190.642073	5342.280870	25.879834
190.553342	5375.288543	25.884852
190.689783	5365.427252	25.889869
191.049067	5378.830427	25.894887
190.618101	5380.423223	25.899904
191.383889	5379.423311	25.904922
191.189956	5408.560563	25.909940
191.422083	5396.119228	25.914957
191.497422	5418.685219	25.919975
191.711291	5419.178414	25.924992
192.496066	5427.473946	25.930010
192.101998	5445.582410	25.935028
192.811302	5450.383485	25.940045
192.845594	5456.577714	25.945063
193.114922	5461.432418	25.950080
193.321379	5463.337424	25.955098
193.401484	5468.864278	25.960116
193.539488	5487.327753	25.965133
193.964218	5488.742439	25.970151
193.898132	5482.527656	25.975168
194.497436	5491.966036	25.980186
194.589831	5509.561952	25.985204
194.788879	5500.600852	25.990221
195.409143	5502.840343	25.995239
194.907888	5507.791166	26.000256
195.328184	5499.972549	26.005274
195.254678	5522.184005	26.010292
195.769160	5523.885709	26.015309
195.891355	5539.297626	26.020327
195.789479	5530.837650	26.025344
196.165816	5544.205214	26.030362
196.033659	5560.754429	26.035380
196.372345	5553.829951	26.040397
196.692326	5577.703306	26.045415
196.327160	5592.512440	26.050432
196.873763	5593.428578	26.055450
197.260751	5616.443197	26.060468
197.620832	5624.984357	26.065485
197.847914	5615.293336	26.070503
197.816131	5636.896448	26.075520
198.333657	5627.863256	26.080538
198.241354	5646.634289	26.085556
198.613641	5645.280120	26.090573
198.917841	5652.559603	26.095591
198.787091	5673.110924	26.100608
199.469103	5654.254850	26.105626
199.393998	5655.560421	26.110644
199.493650	5662.168376	26.115661
199.793048	5686.547923	26.120679
200.193204	5690.851573	26.125696
200.038835	5685.806521	26.130714
200.110672	5695.272480	26.135732
200.421636	5710.723716	26.140749
201.030391	5710.799927	26.145767
200.632538	5722.328128	26.150784
200.998228	5716.246606	26.155802
201.325908	5740.748401	26.160820
201.102913	5737.782655	26.165837
201.285432	5742.829885	26.170855
201.241210	5751.360835	26.175872
201.846532	5768.920917	26.180890
202.044560	5775.024662	26.185908
202.166707	5786.837427	26.190925
202.545394	5796.672300	26.195943
203.050972	5804.541293	26.200960
203.138212	5811.543101	26.205978
203.308000	5821.153237	26.210996
203.474953	5822.781355	26.216013
203.617251	5833.528031	26.221031
203.614662	5834.223331	26.226048
204.285270	5848.642578	26.231066
203.993162	5860.762981	26.236084
203.953105	5861.753784	26.241101
204.774404	5859.021201	26.246119
204.732304	5882.749790	26.251136
204.897996	5880.153194	26.256154
205.010820	5895.046139	26.261172
205.258287	5909.734317	26.266189
205.407071	5916.796384	26.271207
205.480252	5927.914487	26.276224
206.294829	5939.063886	26.281242
206.086495	5947.020808	26.286260
206.272411	5964.120067	26.291277
206.840396	5958.485339	26.296295
206.908750	5978.145404	26.301312
207.284473	5972.849735	26.306330
207.477840	5971.295900	26.311348
207.705378	5985.493240	26.316365
207.852813	5989.692505	26.321383
208.028687	6001.139682	26.326400
208.107618	5990.044048	26.331418
208.462829	6010.920403	26.336436
208.810889	6015.623482	26.341453
208.910239	6020.243475	26.346471
208.651845	6030.377551	26.351488
209.122871	6040.296214	26.356506
209.136150	6050.098247	26.361524
209.427729	6048.299796	26.366541
209.945873	6066.637303	26.371559
209.699806	6083.873232	26.376576
210.202948	6074.603672	26.381594
210.474283	6096.115858	26.386612
210.542571	6093.779441	26.391629
210.700633	6090.477501	26.396647
210.951252	6121.277761	26.401664
211.762601	6116.498741	26.406682
211.681772	6120.328457	26.411700
212.035890	6112.183332	26.416717
212.124771	6117.935623	26.421735
211.947159	6132.122951	26.426752
212.777686	6119.167834	26.431770
212.531472	6137.846797	26.436788
212.761220	6133.976381	26.441805
213.009462	6141.375177	26.446823
213.351911	6152.142104	26.451840
213.274572	6161.732853	26.456858
213.468205	6163.472413	26.461876
213.285142	6177.322337	26.466893
213.933372	6175.383616	26.471911
214.094745	6198.992941	26.476928
214.299717	6204.426995	26.481946
214.523310	6207.431648	26.486964
214.378451	6218.645312	26.491981
215.009879	6216.389831	26.496999
214.901453	6233.789670	26.502016
215.079690	6242.899915	26.507034
214.956049	6260.025264	26.512052
215.711928	6277.939611	26.517069
215.942436	6293.797677	26.522087
215.289098	6299.459866	26.527104
215.874714	6312.599644	26.532122
216.704780	6322.480143	26.537140
216.779646	6353.157054	26.542157
217.026637	6344.044609	26.547175
217.250142	6368.062870	26.552192
217.685201	6363.767843	26.557210
217.460728	6380.187918	26.562228
217.829406	6392.978399	26.567245
218.369089	6395.922472	26.572263
218.344753	6409.920403	26.577280
218.731970	6417.954941	26.582298
219.032203	6430.089166	26.587316
219.035673	6426.515177	26.592333
219.298285	6442.854523	26.597351
219.548127	6461.353314	26.602368
219.638234	6466.485551	26.607386
219.612370	6468.065802	26.612404
220.021617	6480.789308	26.617421
220.604517	6475.975787	26.622439
220.630686	6498.172815	26.627456
221.072523	6493.448654	26.632474
221.700781	6509.551181	26.637492
221.542429	6501.904545	26.642509
222.034677	6493.248592	26.647527
222.280142	6486.462861	26.652544
222.794350	6494.880036	26.657562
222.957204	6516.263785	26.662580
222.863787	6507.229898	26.667597
223.313167	6502.137884	26.672615
223.461569	6498.760289	26.677632
223.401391	6508.125862	26.682650
223.625607	6513.893711	26.687668
223.423658	6513.362736	26.692685
223.917242	6510.058358	26.697703
223.587521	6537.356338	26.702720
223.671132	6542.510881	26.707738
224.046507	6547.637796	26.712756
223.994451	6563.115540	26.717773
224.249579	6574.848725	26.722791
224.287328	6596.692355	26.727808
224.595853	6597.510404	26.732826
225.150198	6620.030191	26.737844
224.993977	6642.302145	26.742861
225.549722	6652.878862	26.747879
225.862279	6669.695957	26.752896
226.270944	6679.647812	26.757914
226.588218	6690.548971	26.762932
226.518817	6701.607770	26.767949
227.064060	6692.497922	26.772967
227.303064	6722.529427	26.777984
227.129553	6728.018504	26.783002
227.715084	6720.493931	26.788020
228.022996	6745.584358	26.793037
228.182685	6734.935577	26.798055
228.284951	6748.667374	26.803072
228.538071	6762.227214	26.808090
229.130441	6763.996913	26.813108
229.010082	6774.903381	26.818125
229.550183	6782.196175	26.823143
229.350437	6804.098428	26.828160
229.409364	6808.593715	26.833178
230.057517	6805.665908	26.838196
230.500020	6829.449369	26.843213
230.731788	6836.074556	26.848231
230.634513	6832.877677	26.853248
230.724293	6848.340188	26.858266
230.889343	6849.221251	26.863284
231.125003	6870.823655	26.868301
231.636224	6886.276459	26.873319
231.913100	6890.868426	26.878336
232.216371	6892.306555	26.883354
232.417289	6903.927475	26.888372
232.511470	6909.038759	26.893389
232.826703	6919.370755	26.898407
232.971767	6927.205770	26.903424
232.902655	6940.278958	26.908442
233.497715	6941.686314	26.913460
233.648790	6946.554855	26.918477
234.028159	6957.953025	26.923495
233.859887	6955.491313	26.928512
234.025238	6980.480546	26.933530
234.657686	6985.420286	26.938548
234.896284	7007.493727	26.943565
235.140585	7006.192895	26.948583
235.248220	7017.938143	26.953600
235.682061	7019.262626	26.958618
235.801411	7032.907772	26.963636
235.736310	7052.181388	26.968653
236.361450	7044.873012	26.973671
236.346738	7072.530905	26.978688
236.686236	7069.443744	26.983706
237.224689	7075.597623	26.988724
237.443214	7091.253094	26.993741
237.525117	7102.693288	26.998759
237.931554	7092.745323	27.003776
237.842607	7095.343623	27.008794
238.275368	7082.352739	27.013812
238.495574	7104.059447	27.018829
238.816173	7105.055786	27.023847
238.549403	7122.880830	27.028864
238.994448	7125.666254	27.033882
239.239399	7141.811694	27.038900
239.196038	7150.247316	27.043917
239.274918	7157.673623	27.048935
239.824553	7166.549769	27.053952
239.819737	7175.530044	27.058970
240.082078	7182.521898	27.063988
240.165722	7207.292423	27.069005
240.432784	7229.236550	27.074023
240.833341	7230.667074	27.079040
241.120885	7263.334918	27.084058
241.413825	7259.582395	27.089076
241.744391	7276.189584	27.094093
242.167449	7295.111876	27.099111
242.318049	7303.172817	27.104128
242.244954	7308.764124	27.109146
242.868561	7324.702263	27.114164
242.658128	7340.664003	27.119181
242.983798	7345.045329	27.124199
243.286925	7360.248934	27.129216
243.593306	7386.490266	27.134234
244.020049	7387.557832	27.139252
244.443389	7399.925808	27.144269
244.593394	7412.575779	27.149287
244.712179	7418.492981	27.154304
245.108800	7418.539305	27.159322
245.797579	7440.141123	27.164340
245.523343	7448.378450	27.169357
245.743027	7450.020378	27.174375
245.862402	7468.553815	27.179392
245.965941	7482.836882	27.184410
246.274401	7475.234142	27.189428
246.592703	7499.388627	27.194445
246.662649	7506.851153	27.199463
247.008349	7526.338441	27.204480
247.473785	7532.659164	27.209498
247.883189	7544.052212	27.214516
248.168667	7561.453760	27.219533
248.323162	7557.482456	27.224551
248.583634	7578.385570	27.229568
248.501968	7594.503310	27.234586
249.028532	7597.866759	27.239604
249.108130	7616.496423	27.244621
249.501882	7623.365247	27.249639
249.402229	7639.715665	27.254656
249.743359	7642.804170	27.259674
250.011178	7651.353351	27.264692
249.874769	7669.355766	27.269709
250.506135	7677.279685	27.274727
250.576675	7693.668341	27.279744
251.021099	7701.142088	27.284762
251.497488	7706.855258	27.289780
251.688823	7717.076944	27.294797
251.894858	7730.815927	27.299815
252.234326	7733.977108	27.304832
252.197073	7746.661936	27.309850
252.504208	7743.545963	27.314868
252.796215	7775.634304	27.319885
253.274977	7766.709092	27.324903
253.788380	7777.760768	27.329920
253.816971	7788.935373	27.334938
254.262188	7790.311624	27.339956
254.064954	7788.703415	27.344973
254.414174	7807.801801	27.349991
254.778181	7811.865558	27.355008
254.829148	7822.296966	27.360026
255.259260	7828.142672	27.365044
255.609659	7852.827685	27.370061
255.530052	7857.221834	27.375079
256.066902	7863.467580	27.380096
255.769186	7881.456621	27.385114
255.980971	7887.721932	27.390132
256.283441	7899.057548	27.395149
255.995005	7915.267609	27.400167
256.888033	7934.539140	27.405184
256.927963	7956.783363	27.410202
257.454986	7959.503949	27.415220
257.376217	7994.559363	27.420237
257.399446	8007.717913	27.425255
257.927947	8021.713431	27.430272
258.242389	8044.392448	27.435290
258.925506	8053.801817	27.440308
259.574193	8077.307335	27.445325
259.393494	8092.394060	27.450343
259.898446	8094.180228	27.455360
260.239738	8117.944907	27.460378
260.470040	8115.818415	27.465396
260.765849	8112.697091	27.470413
260.698831	8133.630369	27.475431
261.284606	8144.386720	27.480448
261.722188	8142.630854	27.485466
261.562086	8152.298238	27.490484
261.930911	8166.288657	27.495501
262.184896	8163.901859	27.500519
262.736905	8188.980210	27.505536
262.593557	8213.793705	27.510554
263.011863	8198.262910	27.515572
263.377740	8226.550409	27.520589
263.298738	8234.934489	27.525607
263.545724	8228.416452	27.530624
263.970097	8249.142907	27.535642
264.147812	8260.375537	27.540660
264.187327	8268.513333	27.545677
264.478737	8289.266153	27.550695
264.849666	8291.483680	27.555712
264.753705	8314.506300	27.560730
265.411713	8317.793491	27.565748
265.678492	8320.597335	27.570765
265.803151	8349.579786	27.575783
266.135548	8348.770380	27.580800
266.065103	8366.294523	27.585818
266.638828	8370.779832	27.590836
266.617009	8385.869069	27.595853
266.836727	8407.165423	27.600871
267.243178	8415.756686	27.605888
267.073268	8440.274589	27.610906
267.790876	8452.768870	27.615924
268.162980	8465.503157	27.620941
268.557481	8479.924935	27.625959
269.178508	8491.368393	27.630976
269.063765	8498.625965	27.635994
269.632024	8506.499408	27.641012
270.017065	8522.977733	27.646029
270.395002	8515.829636	27.651047
270.623479	8525.092231	27.656064
270.733900	8552.317436	27.661082
270.783093	8562.991225	27.666100
271.305098	8562.346345	27.671117
271.479561	8587.120423	27.676135
271.828921	8582.740861	27.681152
271.690604	8598.689691	27.686170
272.357097	8608.827989	27.691188
272.374626	8610.975205	27.696205
272.377622	8626.543890	27.701223
273.010285	8643.723360	27.706240
273.006327	8669.828745	27.711258
273.350991	8662.744507	27.716276
273.428168	8689.979982	27.721293
273.772617	8702.876263	27.726311
273.962792	8721.048222	27.731328
274.351627	8726.885128	27.736346
274.740413	8758.592275	27.741364
275.135104	8759.245634	27.746381
275.401112	8774.303154	27.751399
276.062039	8785.532735	27.756416
275.651985	8804.149073	27.761434
275.902574	8811.861634	27.766452
276.465130	8816.138755	27.771469
276.939473	8837.378218	27.776487
277.471185	8849.086431	27.781504
277.254261	8855.147424	27.786522
278.028539	8861.709080	27.791540
278.200371	8878.201716	27.796557
278.049854	8889.285687	27.801575
278.993301	8887.676135	27.806592
278.906021	8899.989831	27.811610
278.949055	8917.543746	27.816628
279.442105	8915.367787	27.821645
279.423213	8938.304717	27.826663
279.746142	8928.552602	27.831680
279.937426	8947.513945	27.836698
280.253765	8957.576093	27.841716
280.415882	8971.595104	27.846733
280.487024	8993.242552	27.851751
280.871774	8991.785391	27.856768
281.054598	9033.396001	27.861786
281.488307	9032.695142	27.866804
281.844447	9051.250253	27.871821
282.024823	9058.491745	27.876839
282.227581	9074.814020	27.881856
282.483858	9088.669402	27.886874
283.161113	9108.383310	27.891892
283.694559	9111.361208	27.896909
283.836435	9126.572649	27.901927
283.866950	9143.442223	27.906944
284.096311	9153.859505	27.911962
284.408151	9167.069472	27.916980
284.710795	9181.927584	27.921997
284.954410	9192.863180	27.927015
285.422441	9212.658185	27.932032
285.402139	9226.675427	27.937050
285.718297	9240.716961	27.942068
286.083307	9261.822970	27.947085
286.114559	9278.806292	27.952103
286.611371	9286.941003	27.957120
286.408900	9306.706077	27.962138
286.949394	9327.280563	27.967156
287.328061	9338.755045	27.972173
287.726285	9353.767287	27.977191
288.037772	9373.667332	27.982208
288.361062	9399.026951	27.987226
288.647237	9410.598861	27.992244
289.082979	9416.684323	27.997261
289.235251	9443.179695	28.002279
289.532621	9453.763016	28.007296
290.054341	9464.719408	28.012314
290.187831	9491.418532	28.017332
290.424317	9489.829928	28.022349
290.561498	9521.993916	28.027367
290.914968	9536.034502	28.032384
291.020767	9548.180629	28.037402
291.613497	9555.979909	28.042420
292.035233	9584.530610	28.047437
292.071015	9593.423627	28.052455
292.892065	9607.881210	28.057472
293.273479	9606.620086	28.062490
293.529395	9619.826776	28.067508
293.817114	9640.133101	28.072525
294.033699	9641.680158	28.077543
294.353239	9655.544476	28.082560
294.794203	9661.118861	28.087578
295.088321	9664.362059	28.092596
295.087362	9661.355402	28.097613
295.023714	9677.161265	28.102631
295.530300	9681.595905	28.107648
295.598253	9695.804916	28.112666
295.960429	9723.704719	28.117684
296.527077	9715.769706	28.122701
296.547239	9739.732954	28.127719
296.997245	9741.447035	28.132736
297.214490	9753.057347	28.137754
297.324298	9760.365516	28.142772
297.908229	9775.398557	28.147789
297.932152	9788.749007	28.152807
298.664031	9790.938354	28.157824
298.840857	9798.678531	28.162842
298.426787	9828.188839	28.167860
299.312683	9829.228668	28.172877
299.086023	9857.357932	28.177895
299.574252	9863.829093	28.182912
299.534862	9896.937278	28.187930
299.742159	9917.484627	28.192948
300.178840	9932.032514	28.197965
300.386163	9968.514261	28.202983
300.979009	9983.574422	28.208000
301.523894	9997.590048	28.213018
302.018363	10015.508496	28.218036
302.301879	10018.868362	28.223053
302.291144	10044.187873	28.228071
302.828366	10051.394221	28.233088
302.940880	10079.182196	28.238106
303.540365	10094.029711	28.243124
304.011321	10115.641023	28.248141
303.984992	10130.186562	28.253159
304.467227	10137.167980	28.258176
304.907487	10154.919737	28.263194
304.889268	10174.377199	28.268212
305.382775	10181.487088	28.273229
305.421761	10201.504462	28.278247
305.988785	10212.721369	28.283264
306.479266	10239.166601	28.288282
306.415304	10249.296925	28.293300
307.147740	10247.029903	28.298317
306.980571	10278.381473	28.303335
307.564517	10281.170557	28.308352
308.257610	10296.749033	28.313370
308.303481	10307.565465	28.318388
308.628915	10315.013070	28.323405
308.591995	10334.546124	28.328423
309.185822	10354.321412	28.333440
309.446081	10368.368979	28.338458
309.376783	10368.151971	28.343476
309.856554	10392.414075	28.348493
309.895174	10416.675305	28.353511
310.311715	10432.302722	28.358528
310.525672	10448.930853	28.363546
310.423781	10458.778138	28.368564
311.103096	10478.053595	28.373581
311.127346	10500.743239	28.378599
312.041636	10508.042784	28.383616
312.393229	10538.533470	28.388634
312.400697	10547.333188	28.393652
312.728100	10550.583869	28.398669
312.941347	10579.351099	28.403687
313.020149	10594.340732	28.408704
313.318093	10618.881664	28.413722
313.726489	10633.351712	28.418740
314.281528	10657.868849	28.423757
314.275882	10682.850993	28.428775
314.825480	10694.727019	28.433792
315.327954	10719.025776	28.438810
315.358085	10740.180157	28.443828
315.749347	10751.130350	28.448845
315.892571	10768.041235	28.453863
316.572231	10772.092889	28.458880
316.766965	10799.432292	28.463898
317.057013	10822.434217	28.468916
317.765278	10837.221455	28.473933
317.798415	10855.050339	28.478951
318.231561	10872.590796	28.483968
318.270884	10888.420080	28.488986
318.538095	10915.310948	28.494004
319.240010	10915.155181	28.499021
319.541896	10948.493038	28.504039
319.449750	10961.996428	28.509056
319.898578	10980.361681	28.514074
320.356984	11002.649970	28.519092
321.070638	11019.129044	28.524109
320.980262	11039.780067	28.529127
321.336690	11050.696286	28.534144
321.902687	11064.804387	28.539162
322.143596	11081.178250	28.544180
322.784665	11093.369390	28.549197
322.840274	11104.186809	28.554215
323.317395	11120.253113	28.559232
323.592008	11132.257527	28.564250
323.791403	11151.323069	28.569268
323.976627	11168.512224	28.574285
324.106517	11194.580980	28.579303
324.563521	11200.583903	28.584320
325.024493	11217.779932	28.589338
324.908099	11245.899320	28.594356
325.651266	11255.794643	28.599373
326.043663	11271.217427	28.604391
326.172407	11291.653637	28.609408
326.977037	11305.513399	28.614426
326.886463	11317.857926	28.619444
327.237504	11334.503752	28.624461
327.547255	11353.497655	28.629479
328.352146	11374.348031	28.634496
328.652372	11378.285208	28.639514
328.382527	11394.355549	28.644532
328.917495	11403.912663	28.649549
329.273400	11421.799389	28.654567
329.533986	11440.330578	28.659584
329.837334	11441.998192	28.664602
330.021814	11468.929992	28.669620
330.279819	11474.170993	28.674637
330.532188	11496.552471	28.679655
330.767463	11509.197628	28.684672
331.180618	11528.830893	28.689690
331.459443	11554.143976	28.694708
331.689123	11564.208901	28.699725
332.183199	11592.732605	28.704743
332.486823	11612.424953	28.709760
332.907804	11627.582636	28.714778
332.976330	11648.330371	28.719796
333.690266	11666.947394	28.724813
333.892422	11692.913405	28.729831
334.257972	11713.412993	28.734848
334.517936	11723.071201	28.739866
334.472810	11753.801906	28.744884
335.101787	11768.431513	28.749901
335.478929	11787.349108	28.754919
335.847022	11815.064128	28.759936
336.440428	11824.609050	28.764954
336.757153	11847.818043	28.769972
337.226255	11861.366984	28.774989
337.803404	11880.807318	28.780007
338.079595	11906.445884	28.785024
338.229623	11905.713975	28.790042
338.460679	11927.230945	28.795060
338.904521	11931.132196	28.800077
339.370030	11947.678207	28.805095
339.514476	11973.841616	28.810112
339.888351	11989.126610	28.815130
339.841284	12006.817726	28.820148
339.916014	12031.690506	28.825165
340.440679	12050.786808	28.830183
340.354720	12079.475300	28.835200
341.640950	12111.005174	28.840218
341.647354	12128.793183	28.845236
342.193255	12147.679022	28.850253
342.570376	12162.972726	28.855271
342.572724	12191.824059	28.860288
343.394294	12196.151805	28.865306
343.790982	12228.508265	28.870324
343.888490	12240.993974	28.875341
344.448600	12270.320326	28.880359
344.616213	12278.597885	28.885376
345.165272	12291.488656	28.890394
345.373577	12313.082999	28.895412
345.873488	12330.389797	28.900429
346.351016	12342.283536	28.905447
346.563913	12367.986100	28.910464
346.870015	12370.459180	28.915482
346.719686	12402.035995	28.920500
347.168727	12393.185430	28.925517
347.379922	12427.614810	28.930535
347.825149	12439.295942	28.935552
348.372530	12447.375131	28.940570
348.365949	12471.320601	28.945588
348.915413	12497.141337	28.950605
349.318392	12499.098003	28.955623
349.637368	12516.487963	28.960640
349.969022	12534.335006	28.965658
349.967320	12553.345617	28.970676
350.517954	12573.716518	28.975693
351.263821	12598.182200	28.980711
351.195193	12609.207826	28.985728
351.930523	12632.437501	28.990746
351.865157	12645.893057	28.995764
352.420757	12662.440647	29.000781
353.229262	12685.428510	29.005799
353.264956	12706.775823	29.010816
353.545581	12724.520829	29.015834
353.842841	12733.040678	29.020852
354.598399	12758.830394	29.025869
354.855508	12776.565434	29.030887
354.887983	12799.104507	29.035904
355.525034	12797.965336	29.040922
355.871601	12828.886099	29.045940
355.699326	12840.848759	29.050957
356.180818	12857.854675	29.055975
356.289114	12881.052618	29.060992
356.974272	12902.908307	29.066010
357.412727	12928.587681	29.071028
357.827029	12946.615477	29.076045
358.316947	12972.991014	29.081063
357.882515	12992.514881	29.086080
358.556165	13010.925099	29.091098
358.953599	13045.911043	29.096116
359.152422	13068.388387	29.101133
360.043620	13085.380629	29.106151
360.091515	13115.287324	29.111168
360.575039	13136.615038	29.116186
361.001532	13161.999861	29.121204
361.564999	13174.062590	29.126221
362.041078	13190.699981	29.131239
362.245312	13223.424754	29.136256
362.432902	13244.491808	29.141274
362.459270	13250.473859	29.146292
363.283246	13283.307413	29.151309
363.761330	13293.227343	29.156327
363.592583	13324.414050	29.161344
364.475749	13335.183930	29.166362
364.694967	13361.190713	29.171380
365.019286	13382.836572	29.176397
365.469770	13396.479693	29.181415
365.720781	13430.863280	29.186432
366.150158	13428.550546	29.191450
366.599110	13442.062793	29.196468
366.854742	13468.219223	29.201485
367.873621	13477.452098	29.206503
367.619608	13484.164932	29.211520
367.897773	13498.311544	29.216538
368.399646	13511.549753	29.221556
368.694714	13525.901336	29.226573
369.328381	13541.055975	29.231591
369.229379	13569.816161	29.236608
369.781906	13582.529290	29.241626
370.063717	13594.845149	29.246644
370.077239	13627.669863	29.251661
370.752843	13641.987949	29.256679
371.050592	13671.953922	29.261696
371.607199	13682.185222	29.266714
371.521358	13719.274629	29.271732
372.164241	13732.780437	29.276749
372.975363	13751.994118	29.281767
372.721085	13778.764174	29.286784
373.479282	13793.349772	29.291802
373.815416	13814.339332	29.296820
373.989695	13829.786696	29.301837
374.459052	13856.678809	29.306855
374.608884	13867.371697	29.311872
375.137974	13903.337860	29.316890
375.412140	13928.483842	29.321908
375.628017	13943.602439	29.326925
376.239763	13967.437261	29.331943
376.200332	14004.278199	29.336960
376.840115	14021.287355	29.341978
377.523996	14059.998849	29.346996
377.944299	14087.474427	29.352013
378.083714	14107.809995	29.357031
378.516406	14128.811661	29.362048
379.308283	14147.741291	29.367066
379.503274	14165.009725	29.372084
380.023237	14193.938424	29.377101
380.624240	14202.117467	29.382119
380.793735	14234.663182	29.387136
381.095207	14238.125840	29.392154
381.719336	14255.532731	29.397172
382.060158	14279.288411	29.402189
382.360840	14283.952870	29.407207
382.637699	14319.796077	29.412224
382.990017	14322.448589	29.417242
383.215332	14350.333841	29.422260
383.548907	14371.552570	29.427277
383.926361	14391.447633	29.432295
383.970657	14424.368438	29.437312
384.524441	14446.338013	29.442330
385.040395	14466.617698	29.447348
385.201863	14491.665272	29.452365
385.886625	14514.357500	29.457383
386.123081	14547.499660	29.462400
386.803302	14567.246139	29.467418
387.114956	14586.037929	29.472436
387.378899	14604.585435	29.477453
388.176246	14623.917648	29.482471
388.041197	14634.738438	29.487488
388.580850	14656.015550	29.492506
388.811628	14679.327879	29.497524
388.831552	14701.230761	29.502541
389.557020	14718.831830	29.507559
389.783127	14755.371590	29.512576
390.699490	14775.130502	29.517594
390.946557	14794.669391	29.522612
391.173677	14816.154761	29.527629
391.615442	14830.853680	29.532647
391.592595	14851.169547	29.537664
392.067874	14877.795744	29.542682
392.444960	14904.434976	29.547700
392.511727	14934.051829	29.552717
393.016635	14956.363617	29.557735
393.420491	14999.002999	29.562752
393.856407	15022.576408	29.567770
394.387754	15054.017992	29.572788
394.481925	15093.754727	29.577805
395.029024	15116.087481	29.582823
395.367425	15149.714108	29.587840
395.989666	15177.464820	29.592858
396.898037	15211.859453	29.597876
397.080017	15223.064308	29.602893
397.522650	15248.775760	29.607911
397.961543	15278.925797	29.612928
398.196921	15301.443212	29.617946
398.814309	15324.272948	29.622964
399.060215	15351.743161	29.627981
400.269495	15379.036001	29.632999
400.325358	15396.902202	29.638016
400.038047	15408.477193	29.643034
400.759094	15436.563750	29.648052
400.709743	15458.920208	29.653069
401.381373	15486.882176	29.658087
401.845284	15512.346333	29.663104
402.243296	15551.589161	29.668122
402.643352	15561.915170	29.673140
402.761457	15601.057474	29.678157
403.397964	15612.167160	29.683175
403.664747	15653.514474	29.688192
404.058030	15676.569096	29.693210
404.735987	15697.432082	29.698228
405.037582	15726.614977	29.703245
405.765139	15747.340818	29.708263
406.013625	15770.923889	29.713280
406.355513	15790.705493	29.718298
406.912429	15819.146020	29.723316
407.344078	15851.715784	29.728333
408.008358	15863.816749	29.733351
407.985747	15886.232942	29.738368
408.385643	15921.421896	29.743386
408.900436	15935.001446	29.748404
408.978931	15950.553207	29.753421
409.751612	15973.032540	29.758439
410.299354	15996.951882	29.763456
410.478721	16010.916002	29.768474
410.502771	16022.887053	29.773492
410.635257	16058.696803	29.778509
411.232648	16072.568194	29.783527
411.500092	16104.333471	29.788544
411.707517	16128.665464	29.793562
412.629859	16166.655801	29.798580
412.821514	16191.520651	29.803597
413.419051	16219.941867	29.808615
413.637725	16259.205235	29.813632
413.986455	16282.179096	29.818650
414.246165	16314.604817	29.823668
414.302056	16358.263336	29.828685
415.346866	16389.032408	29.833703
415.957799	16420.540677	29.838720
416.189419	16442.655191	29.843738
416.456274	16476.560263	29.848756
417.102752	16496.030491	29.853773
417.758150	16519.206012	29.858791
418.018716	16552.806775	29.863808
418.738817	16577.563836	29.868826
419.386644	16592.546838	29.873844
419.374072	16626.805000	29.878861
420.021500	16646.088081	29.883879
420.230642	16669.069211	29.888896
420.877550	16694.065660	29.893914
421.484824	16723.780227	29.898932
421.556598	16751.988196	29.903949
422.229714	16784.015599	29.908967
422.306404	16806.006711	29.913984
423.151722	16835.381426	29.919002
423.472153	16847.163385	29.924020
423.700654	16882.633791	29.929037
424.142257	16898.980549	29.934055
424.804725	16937.325590	29.939072
425.141685	16956.044405	29.944090
425.779598	16976.260053	29.949108
425.905264	17013.823362	29.954125
426.337610	17020.842113	29.959143
426.831777	17052.255328	29.964160
427.329875	17085.094652	29.969178
427.727664	17095.286043	29.974196
427.782282	17126.128346	29.979213
428.134994	17141.899211	29.984231
428.576803	17176.405461	29.989248
429.416767	17213.956423	29.994266
429.951400	17225.891342	29.999284
430.177052	17258.319747	30.004301
430.774410	17276.068185	30.009319
430.815668	17309.937019	30.014336
431.391624	17333.062649	30.019354
432.097446	17345.132778	30.024372
432.378643	17379.497758	30.029389
432.724179	17385.254000	30.034407
433.236773	17412.153038	30.039424
433.421218	17424.624789	30.044442
433.826499	17454.240474	30.049460
434.250565	17472.614360	30.054477
434.891401	17504.458649	30.059495
434.873866	17527.791332	30.064512
435.099127	17563.285664	30.069530
435.828647	17593.595594	30.074548
435.954863	17629.112943	30.079565
435.936430	17639.047598	30.084583
437.022639	17686.074714	30.089600
437.296523	17716.779913	30.094618
437.715088	17747.196380	30.099636
438.059191	17790.811442	30.104653
438.746533	17816.180229	30.109671
439.218489	17854.263419	30.114688
439.725440	17889.753773	30.119706
440.482903	17915.895001	30.124724
440.581081	17952.085261	30.129741
440.946938	17973.823693	30.134759
441.841219	18010.378187	30.139776
442.206618	18030.355373	30.144794
443.059470	18052.206873	30.149812
443.141842	18088.979887	30.154829
443.548176	18099.829832	30.159847
443.939759	18130.569852	30.164864
444.461577	18155.864783	30.169882
445.033275	18179.384090	30.174900
445.669899	18206.625379	30.179917
446.022433	18230.122202	30.184935
446.485780	18255.461650	30.189952
446.547847	18288.563551	30.194970
447.475306	18300.739673	30.199988
447.376955	18341.968098	30.205005
448.145182	18356.790135	30.210023
448.650589	18386.065660	30.215040
448.768441	18424.438560	30.220058
449.661335	18438.577811	30.225076
450.006535	18480.583980	30.230093
450.065980	18504.132244	30.235111
450.817123	18520.263880	30.240128
450.998995	18555.122495	30.245146
451.703663	18576.486131	30.250164
451.570138	18609.502550	30.255181
452.845333	18645.926202	30.260199
453.734521	18669.414176	30.265216
453.451365	18694.200026	30.270234
454.218143	18702.662970	30.275252
454.629853	18753.392251	30.280269
454.871513	18769.017503	30.285287
455.184706	18791.887562	30.290304
455.641596	18820.912178	30.295322
456.064838	18838.185016	30.300340
456.404441	18862.868372	30.305357
456.901580	18892.420591	30.310375
457.429568	18920.747815	30.315392
457.825760	18934.732001	30.320410
458.526880	18956.607381	30.325428
458.773242	18986.031220	30.330445
459.150418	19025.143852	30.335463
459.911427	19037.478583	30.340480
459.959505	19067.185361	30.345498
460.170998	19083.019682	30.350516
460.672994	19137.218708	30.355533
461.070127	19158.402602	30.360551
461.894836	19183.723398	30.365568
461.841305	19218.538318	30.370586
462.462052	19255.200750	30.375604
462.586578	19289.635074	30.380621
463.152401	19324.642915	30.385639
463.677569	19363.434370	30.390656
464.291769	19400.191107	30.395674
464.815224	19434.205079	30.400692
465.091168	19490.176917	30.405709
465.607338	19508.170402	30.410727
466.598263	19543.722479	30.415744
467.021734	19591.459438	30.420762
467.631580	19610.233859	30.425780
468.291183	19636.046700	30.430797
468.398869	19667.712628	30.435815
468.957867	19702.027850	30.440832
469.284079	19726.140634	30.445850
469.835512	19749.780917	30.450868
470.269630	19794.935439	30.455885
470.828737	19816.798040	30.460903
471.484370	19843.730479	30.465920
471.913734	19887.485090	30.470938
472.276645	19902.754723	30.475956
473.203173	19928.924388	30.480973
473.459214	19956.032899	30.485991
474.017183	19983.329998	30.491008
474.400416	20020.718369	30.496026
474.714967	20034.223973	30.501044
475.213404	20069.302102	30.506061
475.396296	20108.825217	30.511079
476.030286	20136.599115	30.516096
476.273541	20170.785726	30.521114
477.154695	20203.005190	30.526132
477.660283	20234.644311	30.531149
478.200115	20270.996782	30.536167
478.691214	20299.990352	30.541184
478.678925	20319.062406	30.546202
479.554357	20343.982076	30.551220
479.889195	20385.824921	30.556237
480.467575	20426.530888	30.561255
480.882712	20446.369769	30.566272
480.705763	20477.474323	30.571290
481.467277	20507.693101	30.576308
481.928297	20535.526371	30.581325
482.544549	20563.159344	30.586343
483.145658	20595.283660	30.591360
483.473338	20630.762356	30.596378
483.919413	20649.262892	30.601396
484.171860	20690.462484	30.606413
484.565653	20713.129573	30.611431
485.314233	20756.828671	30.616448
485.844354	20788.259064	30.621466
486.499114	20820.324892	30.626484
486.972862	20849.818392	30.631501
487.163751	20883.406526	30.636519
487.580197	20901.294651	30.641536
488.204462	20954.970170	30.646554
488.947469	20971.464382	30.651572
489.447470	21021.486042	30.656589
489.532932	21048.713004	30.661607
490.316175	21073.158278	30.666624
490.503834	21116.570503	30.671642
491.052969	21147.525269	30.676660
491.698541	21193.551881	30.681677
492.052085	21230.482422	30.686695
492.776749	21264.960543	30.691712
492.691123	21306.557405	30.696730
493.449410	21339.315818	30.701748
493.942696	21388.464735	30.706765
494.290245	21424.644564	30.711783
494.875414	21461.319804	30.716800
495.071682	21507.696135	30.721818
495.868968	21545.370282	30.726836
496.895752	21579.861609	30.731853
497.138675	21629.381942	30.736871
498.134118	21652.312890	30.741888
498.260072	21693.258031	30.746906
498.841096	21727.628524	30.751924
499.213816	21763.837413	30.756941
499.385545	21800.644676	30.761959
500.461340	21831.060880	30.766976
500.670359	21871.667192	30.771994
500.950420	21909.227710	30.777012
501.441749	21947.853351	30.782029
501.818093	21976.122451	30.787047
502.855687	22025.073232	30.792064
502.953443	22061.989761	30.797082
503.507558	22106.402500	30.802100
504.595874	22128.975170	30.807117
505.133005	22173.289990	30.812135
505.634768	22196.131044	30.817152
506.274734	22220.003929	30.822170
506.985561	22255.883638	30.827188
507.228029	22283.974564	30.832205
507.647091	22311.535702	30.837223
508.512385	22333.662180	30.842240
508.418014	22377.422879	30.847258
508.922464	22391.289738	30.852276
509.941232	22414.707195	30.857293
509.855264	22450.657568	30.862311
510.661704	22474.605136	30.867328
510.682796	22503.399616	30.872346
511.431910	22529.298666	30.877364
511.543081	22572.976756	30.882381
511.936711	22610.790218	30.887399
512.817188	22639.489792	30.892416
512.889662	22667.963698	30.897434
513.737952	22708.522309	30.902452
514.171758	22742.083580	30.907469
514.608202	22781.494245	30.912487
515.096498	22811.260836	30.917504
515.561092	22841.252584	30.922522
516.116895	22888.115223	30.927540
516.945307	22921.906230	30.932557
517.285023	22962.669379	30.937575
517.696786	23002.573651	30.942592
517.991249	23045.448016	30.947610
518.742858	23086.095460	30.952628
519.532928	23123.854874	30.957645
519.651499	23167.409760	30.962663
520.342115	23200.797983	30.967680
520.776844	23241.610513	30.972698
521.376507	23281.128748	30.977716
521.889836	23329.620456	30.982733
522.519550	23361.767129	30.987751
523.286056	23395.882501	30.992768
523.298520	23446.371521	30.997786
524.198294	23484.107231	31.002804
524.695165	23518.168934	31.007821
524.919050	23572.009287	31.012839
525.832145	23599.423871	31.017856
526.531273	23644.582659	31.022874
526.973105	23677.127744	31.027892
527.258321	23720.510305	31.032909
527.766988	23762.564019	31.037927
528.444033	23778.428160	31.042944
528.934860	23841.366375	31.047962
529.385592	23872.747821	31.052980
530.415991	23894.790330	31.057997
530.331661	23950.398218	31.063015
531.157080	23971.635384	31.068032
532.218883	24018.735051	31.073050
532.302939	24045.681456	31.078068
532.707265	24077.236902	31.083085
533.384195	24121.623914	31.088103
534.031671	24167.565150	31.093120
534.062428	24195.266250	31.098138
534.728365	24232.934651	31.103156
535.040033	24279.346395	31.108173
535.714758	24327.093111	31.113191
536.176967	24358.354744	31.118208
536.788220	24398.890062	31.123226
537.237465	24437.490667	31.128244
537.640456	24462.477556	31.133261
538.079709	24508.837348	31.138279
538.941197	24538.275974	31.143296
539.548600	24582.202714	31.148314
540.147838	24615.117720	31.153332
541.108476	24645.749119	31.158349
541.167931	24681.669549	31.163367
541.459908	24719.785442	31.168384
542.182590	24750.314730	31.173402
542.784329	24781.921264	31.178420
543.038843	24821.413232	31.183437
543.364255	24881.500376	31.188455
543.995334	24904.357825	31.193472
544.902763	24945.490151	31.198490
545.500735	25001.289206	31.203508
546.109313	25032.405959	31.208525
546.432596	25068.651535	31.213543
546.577589	25115.302585	31.218560
547.516822	25153.821364	31.223578
547.538310	25191.880636	31.228596
548.453802	25242.994044	31.233613
549.044016	25300.724589	31.238631
549.939160	25326.060616	31.243648
550.152765	25375.856467	31.248666
550.455907	25427.863640	31.253684
551.754627	25469.544722	31.258701
551.835546	25509.885315	31.263719
552.391572	25568.970142	31.268736
553.085486	25598.866756	31.273754
553.347585	25635.517247	31.278772
553.801649	25689.067322	31.283789
554.131194	25740.478109	31.288807
555.351262	25779.513777	31.293824
555.835795	25832.459190	31.298842
556.311355	25879.306386	31.303860
557.347667	25907.495482	31.308877
557.623782	25948.775064	31.313895
558.141346	25988.620331	31.318912
558.987413	26033.013293	31.323930
559.705911	26077.421183	31.328948
560.494652	26104.045321	31.333965
560.779792	26141.511030	31.338983
561.412560	26173.022415	31.344000
561.921227	26214.060812	31.349018
562.223129	26254.450009	31.354036
562.988097	26288.801867	31.359053
563.320592	26332.087873	31.364071
563.817296	26371.564781	31.369088
564.382764	26411.503520	31.374106
564.820947	26463.326312	31.379124
565.334581	26501.784564	31.384141
566.022241	26548.651928	31.389159
566.583681	26594.708382	31.394176
567.408714	26627.968148	31.399194
567.949706	26673.005492	31.404212
568.403532	26697.453632	31.409229
568.784003	26737.016128	31.414247
569.295832	26768.384866	31.419264
569.685478	26808.824506	31.424282
570.044218	26845.615204	31.429300
571.002134	26888.103498	31.434317
571.250783	26937.804854	31.439335
571.761849	26977.732394	31.444352
572.654392	27024.488941	31.449370
572.728749	27073.566143	31.454388
573.179237	27114.178063	31.459405
573.762666	27172.522273	31.464423
574.397737	27219.112402	31.469440
575.286447	27259.392538	31.474458
576.059972	27317.838568	31.479476
576.957666	27339.598159	31.484493
577.233642	27397.165689	31.489511
577.718840	27429.537386	31.494528
578.584610	27488.604359	31.499546
579.091377	27532.628486	31.504564
579.884113	27571.853193	31.509581
580.401075	27616.444765	31.514599
580.704681	27665.405313	31.519616
581.250410	27699.661957	31.524634
581.584337	27764.249399	31.529652
582.336450	27794.864899	31.534669
582.727238	27853.337583	31.539687
583.439375	27903.899369	31.544704
584.158320	27950.308068	31.549722
584.559349	28008.050099	31.554740
584.978312	28053.399100	31.559757
585.750560	28106.482651	31.564775
586.174951	28164.546130	31.569792
586.919943	28212.147460	31.574810
587.544766	28274.367881	31.579828
588.319524	28308.898197	31.584845
588.672253	28370.888134	31.589863
589.144967	28421.012196	31.594880
590.294451	28459.146929	31.599898
590.843130	28513.625781	31.604916
591.460965	28554.448679	31.609933
592.002648	28596.137909	31.614951
592.435257	28643.014947	31.619968
593.191879	28696.449606	31.624986
593.565441	28745.367607	31.630004
594.255797	28788.388884	31.635021
595.150063	28837.704870	31.640039
595.701205	28887.253725	31.645056
596.256736	28933.850432	31.650074
596.725957	28975.766498	31.655092
597.644959	29019.647069	31.660109
598.351526	29064.001263	31.665127
598.777436	29112.442420	31.670144
599.649416	29157.397728	31.675162
599.988989	29193.809937	31.680180
600.659753	29221.005650	31.685197
601.047292	29253.708577	31.690215
601.085583	29305.743631	31.695232
602.260256	29337.897451	31.700250
602.493878	29395.693140	31.705268
602.997200	29424.152951	31.710285
603.442150	29473.324951	31.715303
603.887816	29521.415900	31.720320
604.554578	29570.716765	31.725338
605.062040	29628.630413	31.730356
605.681670	29675.463308	31.735373
606.403073	29724.500633	31.740391
606.774235	29778.350099	31.745408
608.028396	29823.153403	31.750426
608.114958	29893.192646	31.755444
608.491223	29935.622415	31.760461
609.337584	29988.709775	31.765479
609.790919	30054.771864	31.770496
610.624596	30101.228331	31.775514
611.169171	30175.611739	31.780532
611.732556	30219.036837	31.785549
612.405910	30276.888543	31.790567
612.742517	30338.786097	31.795584
613.324184	30390.238475	31.800602
614.198921	30445.951586	31.805620
615.115938	30507.815660	31.810637
615.541240	30565.889135	31.815655
616.248534	30611.760413	31.820672
617.093698	30674.133009	31.825690
617.329592	30728.533542	31.830708
618.286053	30786.092950	31.835725
618.956711	30841.926594	31.840743
619.179573	30898.835689	31.845760
620.275484	30945.891102	31.850778
620.848064	31002.543128	31.855796
621.449160	31050.481436	31.860813
622.172592	31099.049745	31.865831
622.762712	31163.628775	31.870848
623.672688	31200.537772	31.875866
624.026711	31266.890078	31.880884
625.109059	31308.692429	31.885901
625.470177	31358.141928	31.890919
626.162497	31409.543638	31.895936
626.975766	31447.672738	31.900954
627.576867	31495.648598	31.905972
628.162049	31549.272791	31.910989
628.625489	31589.048235	31.916007
629.069932	31648.987050	31.921024
630.066706	31701.033110	31.926042
630.404029	31744.679510	31.931060
630.755800	31798.461473	31.936077
631.624347	31847.727612	31.941095
632.507015	31890.389150	31.946112
633.315092	31945.069837	31.951130
633.724190	31992.072134	31.956148
634.499982	32025.469030	31.961165
635.465158	32045.389553	31.966183
636.211405	32076.758004	31.971200
636.980215	32119.524959	31.976218
637.345277	32153.198730	31.981236
638.214078	32178.744378	31.986253
638.880462	32211.654700	31.991271
638.808030	32257.795033	31.996288
639.429492	32282.399842	32.001306
639.961400	32339.222151	32.006324
639.884202	32377.800998	32.011341
640.735624	32435.863666	32.016359
641.186986	32491.548697	32.021376
641.826208	32541.000022	32.026394
642.115775	32605.314179	32.031412
642.550325	32668.000901	32.036429
643.258034	32724.564837	32.041447
643.963046	32806.163208	32.046464
644.492201	32865.955827	32.051482
645.285468	32935.804068	32.056500
645.632435	32993.236562	32.061517
646.358620	33073.573451	32.066535
647.352340	33136.615838	32.071552
648.099007	33201.951881	32.076570
648.864676	33269.301223	32.081588
649.886951	33335.922715	32.086605
650.654484	33390.608349	32.091623
650.968450	33443.861023	32.096640
651.600687	33503.975285	32.101658
652.436999	33559.184891	32.106676
652.865118	33626.745493	32.111693
653.818479	33670.938872	32.116711
654.236350	33749.105521	32.121728
655.235103	33794.762718	32.126746
655.879970	33859.181223	32.131764
656.489264	33920.831276	32.136781
657.448232	33966.427499	32.141799
658.087238	34037.279136	32.146816
658.912823	34076.775913	32.151834
659.276029	34129.378215	32.156852
659.696799	34193.327688	32.161869
660.292637	34235.970032	32.166887
660.980768	34306.335776	32.171904
662.015959	34352.308714	32.176922
662.589602	34429.827936	32.181940
663.103625	34484.335274	32.186957
664.013600	34540.171706	32.191975
664.639964	34588.340118	32.196992
665.447786	34651.119929	32.202010
666.198787	34694.039836	32.207028
666.881164	34755.925695	32.212045
667.499794	34804.747029	32.217063
667.635589	34860.655790	32.222080
668.610038	34913.727604	32.227098
669.180488	34972.723560	32.232116
669.687108	35015.077855	32.237133
670.648128	35057.719334	32.242151
670.917963	35122.472023	32.247168
671.728737	35162.359975	32.252186
672.299234	35217.609539	32.257204
673.036722	35273.672957	32.262221
673.556759	35319.134693	32.267239
674.088859	35382.055750	32.272256
675.135109	35432.382587	32.277274
675.780059	35489.443617	32.282292
676.127947	35556.709526	32.287309
677.218446	35597.931841	32.292327
677.484790	35659.373356	32.297344
678.162786	35714.440338	32.302362
678.633238	35772.220631	32.307380
679.308541	35836.306138	32.312397
680.373386	35890.563254	32.317415
680.845047	35955.151448	32.322432
681.970111	36001.981732	32.327450
682.742740	36073.895949	32.332468
682.911089	36134.730497	32.337485
684.065020	36185.909567	32.342503
684.670026	36248.109668	32.347520
685.093505	36306.860989	32.352538
685.568617	36371.177490	32.357556
686.538423	36435.194749	32.362573
687.528956	36486.304584	32.367591
688.373279	36553.158058	32.372608
688.801476	36604.780318	32.377626
689.373867	36665.908769	32.382644
689.848943	36735.235541	32.387661
691.007826	36775.311564	32.392679
691.648656	36855.995599	32.397696
691.964529	36916.385376	32.402714
692.826438	36983.753322	32.407732
693.514146	37042.718984	32.412749
694.220027	37104.964533	32.417767
694.272657	37167.394733	32.422784
695.475391	37226.126099	32.427802
696.084991	37306.101463	32.432820
696.606173	37379.555984	32.437837
697.676874	37438.722203	32.442855
698.386697	37507.355728	32.447872
699.004752	37573.311160	32.452890
699.856600	37638.744003	32.457908
701.038551	37695.771183	32.462925
701.421228	37754.809979	32.467943
702.272635	37813.542574	32.472960
703.126777	37859.513001	32.477978
703.770972	37925.336357	32.482996
704.348354	37985.172736	32.488013
705.299192	38033.785028	32.493031
705.871755	38092.307561	32.498048
706.336982	38153.239304	32.503066
707.032613	38204.013439	32.508084
707.718848	38262.868501	32.513101
708.442810	38313.865508	32.518119
708.817343	38369.257553	32.523136
709.748552	38416.849179	32.528154
710.556734	38467.208840	32.533172
711.103166	38525.919939	32.538189
711.737260	38583.694867	32.543207
712.036082	38642.888870	32.548224
713.270197	38697.471844	32.553242
713.714157	38763.555824	32.558260
714.105752	38812.842814	32.563277
715.231606	38882.347578	32.568295
715.589516	38951.866093	32.573312
716.605121	39020.803979	32.578330
717.569259	39070.360078	32.583348
717.889311	39136.853139	32.588365
718.663624	39196.701867	32.593383
719.594541	39258.405474	32.598400
720.037131	39336.461738	32.603418
720.564476	39403.203516	32.608436
721.447935	39477.052558	32.613453
722.417493	39535.710824	32.618471
722.884205	39610.516151	32.623488
723.833869	39678.379162	32.628506
725.014745	39725.668225	32.633524
725.396451	39796.774332	32.638541
726.169313	39858.278209	32.643559
726.872305	39917.792337	32.648576
727.845764	39994.641190	32.653594
728.321212	40045.148395	32.658612
728.915440	40124.633317	32.663629
729.772585	40181.122935	32.668647
730.389323	40259.795937	32.673664
731.250503	40314.501839	32.678682
732.366758	40382.145593	32.683700
732.517239	40452.299342	32.688717
733.504700	40517.863635	32.693735
734.179762	40578.463158	32.698752
734.965135	40646.980663	32.703770
736.001846	40717.467502	32.708788
736.666066	40780.337165	32.713805
737.696025	40835.803208	32.718823
738.313423	40908.606380	32.723840
739.039030	40966.631882	32.728858
739.769240	41017.071440	32.733876
740.278474	41083.647628	32.738893
741.131332	41152.916538	32.743911
741.604473	41210.081003	32.748928
742.409662	41290.564404	32.753946
743.140303	41358.257644	32.758964
743.404314	41422.855579	32.763981
744.530545	41482.948062	32.768999
745.325763	41572.404638	32.774016
745.946663	41625.784104	32.779034
746.871028	41689.713326	32.784052
747.081480	41752.255066	32.789069
748.141634	41800.938011	32.794087
748.885012	41868.495609	32.799104
749.787230	41921.629343	32.804122
750.364886	41985.700027	32.809140
750.923369	42054.167810	32.814157
751.854971	42118.901802	32.819175
752.648554	42189.332469	32.824192
753.154926	42247.999666	32.829210
754.186077	42332.073045	32.834228
754.419726	42390.929241	32.839245
755.320912	42453.704227	32.844263
755.778667	42540.431179	32.849280
756.559987	42601.740115	32.854298
757.103265	42676.026175	32.859316
758.048737	42756.806386	32.864333
759.263136	42829.005346	32.869351
760.217370	42903.315285	32.874368
760.380128	42982.675520	32.879386
761.720893	43039.149619	32.884404
762.443660	43120.799746	32.889421
762.999976	43193.868360	32.894439
763.734218	43268.624966	32.899456
764.537784	43340.692740	32.904474
765.402351	43408.508365	32.909492
765.992168	43489.408555	32.914509
767.466436	43548.386644	32.919527
768.143494	43631.525908	32.924544
768.483443	43691.517845	32.929562
769.396104	43761.106336	32.934580
770.501434	43829.793787	32.939597
771.764281	43892.276690	32.944615
772.529650	43952.012534	32.949632
773.199937	44018.325210	32.954650
774.283871	44081.253679	32.959668
774.477988	44132.866572	32.964685
775.660409	44195.801862	32.969703
776.437717	44253.514749	32.974720
776.676035	44323.865851	32.979738
777.788008	44394.302143	32.984756
778.476488	44457.140350	32.989773
779.272907	44527.236237	32.994791
779.952406	44588.896510	32.999808
780.436632	44668.960939	33.004826
781.514150	44734.309285	33.009844
782.004655	44811.035703	33.014861
782.753281	44874.039352	33.019879
783.577586	44943.239691	33.024896
784.199510	45023.110318	33.029914
785.153435	45093.249662	33.034932
785.611163	45164.165479	33.039949
786.480741	45242.496018	33.044967
787.143423	45313.048562	33.049984
787.896343	45382.542786	33.055002
788.855514	45449.710899	33.060020
789.379431	45519.024436	33.065037
789.962085	45592.461749	33.070055
791.108617	45648.331690	33.075072
791.839237	45739.933833	33.080090
792.774181	45790.824818	33.085108
793.265762	45861.059774	33.090125
794.021416	45938.184314	33.095143
794.817648	46004.402476	33.100160
795.526394	46086.015123	33.105178
796.374206	46154.263731	33.110196
797.246231	46230.235252	33.115213
797.759434	46297.338794	33.120231
798.848593	46373.645506	33.125248
799.631185	46456.260875	33.130266
800.228591	46535.788952	33.135284
801.100256	46615.431486	33.140301
802.269007	46687.745248	33.145319
802.645744	46770.470868	33.150336
803.616338	46833.455713	33.155354
804.913717	46912.580658	33.160372
805.422538	46996.242307	33.165389
805.919238	47078.536963	33.170407
807.308749	47148.233445	33.175424
807.568484	47239.893132	33.180442
808.364298	47311.196075	33.185460
809.233764	47401.043142	33.190477
810.082324	47475.086508	33.195495
810.929654	47541.135109	33.200512
811.413255	47643.312242	33.205530
812.759305	47711.108968	33.210548
813.530823	47802.005429	33.215565
814.402319	47885.133972	33.220583
815.503765	47959.082325	33.225600
816.222626	48044.674940	33.230618
817.433018	48125.043435	33.235636
818.201625	48192.640484	33.240653
819.055353	48280.535085	33.245671
819.959305	48337.985699	33.250688
820.334166	48424.259662	33.255706
821.055065	48489.536788	33.260724
821.858838	48580.987465	33.265741
822.694311	48651.554306	33.270759
823.693233	48742.791745	33.275776
824.250150	48815.385174	33.280794
825.835465	48889.108944	33.285812
826.446763	48957.658496	33.290829
827.052982	49036.991338	33.295847
828.058629	49097.738315	33.300864
828.828369	49194.561881	33.305882
829.661920	49253.926280	33.310900
830.468234	49341.612805	33.315917
831.122087	49424.060601	33.320935
832.044503	49489.445022	33.325952
832.666294	49574.221097	33.330970
833.521672	49636.947128	33.335988
834.546369	49713.322725	33.341005
835.094162	49785.012760	33.346023
835.814253	49846.713406	33.351040
836.356179	49932.854500	33.356058
837.263166	49996.384579	33.361076
838.350859	50069.889520	33.366093
838.786176	50144.233866	33.371111
839.708960	50216.550731	33.376128
840.107639	50310.018672	33.381146
841.196989	50390.306248	33.386164
842.015946	50474.376746	33.391181
842.855397	50558.867246	33.396199
843.995463	50637.611021	33.401216
844.478592	50734.548528	33.406234
845.746725	50812.366987	33.411252
846.445501	50905.840770	33.416269
847.195982	50983.906465	33.421287
848.307075	51062.808203	33.426304
848.837577	51154.006314	33.431322
850.326631	51232.776063	33.436340
851.039689	51332.413177	33.441357
852.398848	51400.739482	33.446375
853.167063	51466.180937	33.451392
853.719599	51546.855796	33.456410
854.919694	51625.490221	33.461428
855.615233	51704.208449	33.466445
856.521331	51787.191911	33.471463
857.310249	51859.555658	33.476480
858.038825	51948.084738	33.481498
859.133529	52027.286836	33.486516
859.526730	52118.054073	33.491533
860.225480	52198.118410	33.496551
861.317824	52280.307594	33.501568
862.134520	52376.033138	33.506586
863.214984	52445.398777	33.511604
863.740804	52537.008622	33.516621
864.549419	52633.279664	33.521639
865.821193	52717.616838	33.526656
866.234991	52812.998527	33.531674
867.072793	52890.370566	33.536692
868.422832	52975.864265	33.541709
868.705647	53071.656371	33.546727
870.397603	53150.638953	33.551744
870.660141	53245.693503	33.556762
871.734670	53331.570445	33.561780
872.631177	53414.458769	33.566797
873.523958	53507.940433	33.571815
874.491226	53589.151795	33.576832
875.454906	53677.661407	33.581850
876.318135	53770.287463	33.586868
877.210800	53852.878556	33.591885
878.091867	53951.199836	33.596903
878.612639	54028.346280	33.601920
879.381778	54116.087280	33.606938
880.632578	54185.536651	33.611956
881.549537	54270.243699	33.616973
882.074849	54343.618883	33.621991
883.411647	54424.740458	33.627008
884.229460	54494.935391	33.632026
884.956296	54570.305841	33.637044
885.777764	54651.639853	33.642061
886.691220	54734.922909	33.647079
887.665304	54812.136264	33.652096
887.769543	54893.468705	33.657114
888.908152	54975.050401	33.662132
889.875773	55074.424560	33.667149
890.477155	55165.281234	33.672167
891.558305	55248.795629	33.677184
892.233036	55346.402862	33.682202
893.320690	55437.366585	33.687220
894.391237	55523.406034	33.692237
895.198943	55612.729557	33.697255
896.175226	55706.461753	33.702272
897.099846	55795.783347	33.707290
897.992770	55887.471603	33.712308
898.923608	55977.885301	33.717325
899.570685	56072.404106	33.722343
900.678689	56171.515665	33.727360
901.845905	56255.604953	33.732378
902.567824	56368.210877	33.737396
903.556605	56449.886133	33.742413
903.912036	56543.187913	33.747431
905.205329	56639.974385	33.752448
905.810149	56747.960789	33.757466
906.987664	56846.146296	33.762484
908.120792	56933.214684	33.767501
908.706604	57037.313427	33.772519
909.710320	57121.123323	33.777536
910.721547	57230.601065	33.782554
911.823253	57308.546504	33.787572
912.760576	57413.986789	33.792589
913.914529	57509.704557	33.797607
915.114545	57594.284074	33.802624
915.785295	57691.339301	33.807642
916.683094	57764.122743	33.812660
917.684442	57854.089307	33.817677
918.314749	57959.976186	33.822695
919.761937	58036.774244	33.827712
920.172950	58144.086164	33.832730
921.221070	58222.489134	33.837748
922.231796	58326.698005	33.842765
923.127182	58413.085079	33.847783
924.455759	58502.396563	33.852800
924.750761	58589.827129	33.857818
926.086185	58678.667961	33.862836
927.036502	58773.846919	33.867853
927.841716	58864.809376	33.872871
929.023747	58955.238740	33.877888
929.365535	59040.940160	33.882906
930.182251	59124.375297	33.887924
931.120382	59197.325285	33.892941
931.792971	59292.349027	33.897959
932.947061	59365.290568	33.902976
933.403012	59470.026673	33.907994
934.006328	59560.143776	33.913012
935.339563	59656.156672	33.918029
936.439095	59753.163918	33.923047
937.093507	59849.228992	33.928064
938.355287	59927.617791	33.933082
939.323068	60028.584647	33.938100
940.348588	60113.695966	33.943117
941.134233	60215.305344	33.948135
942.557929	60299.081721	33.953152
943.554066	60384.918840	33.958170
944.425268	60481.022129	33.963188
945.358147	60567.650041	33.968205
946.449885	60653.760511	33.973223
947.392875	60745.464850	33.978240
948.368062	60839.643155	33.983258
949.102936	60925.028594	33.988276
950.301576	61022.708681	33.993293
950.817163	61131.041020	33.998311
952.003857	61212.888888	34.003328
952.615974	61310.190160	34.008346
953.818448	61401.496453	34.013364
954.829234	61496.149183	34.018381
955.817741	61586.906265	34.023399
956.687243	61685.718920	34.028416
957.555438	61800.724792	34.033434
958.198431	61887.717526	34.038452
959.585810	61986.683029	34.043469
959.831831	62104.015918	34.048487
960.768918	62190.622221	34.053504
962.329530	62311.811234	34.058522
962.723608	62418.471434	34.063540
964.055857	62513.362323	34.068557
965.167926	62631.902748	34.073575
966.175951	62720.385402	34.078592
966.662100	62835.145732	34.083610
967.705045	62956.569661	34.088628
969.021820	63050.287826	34.093645
969.767368	63156.744682	34.098663
971.062011	63247.596825	34.103680
972.193234	63350.181814	34.108698
973.025304	63465.753032	34.113716
974.242173	63563.958119	34.118733
975.012072	63664.445410	34.123751
976.115606	63771.369819	34.128768
976.981032	63872.259864	34.133786
978.009847	63973.853951	34.138804
979.331837	64067.247875	34.143821
980.077893	64176.738921	34.148839
981.196069	64274.518094	34.153856
982.217312	64358.613399	34.158874
982.826658	64460.971600	34.163892
984.173993	64537.657430	34.168909
985.167500	64638.493256	34.173927
986.079911	64709.052713	34.178944
986.975511	64810.653504	34.183962
987.671321	64896.915768	34.188980
989.155833	64990.642076	34.193997
989.497043	65087.999502	34.199015
990.777472	65175.995458	34.204032
991.674600	65285.216161	34.209050
992.005671	65381.888196	34.214068
993.398869	65479.408701	34.219085
994.146343	65575.769120	34.224103
995.134217	65691.439558	34.229120
995.808659	65795.326311	34.234138
996.657454	65911.130740	34.239156
998.198197	66026.058299	34.244173
998.697529	66134.026920	34.249191
999.821183	66248.469447	34.254208
1001.144235	66354.198444	34.259226
1002.198547	66471.208487	34.264244
1003.295278	66580.786966	34.269261
1004.055562	66692.422064	34.274279
1005.420284	66791.908853	34.279296
1006.021819	66908.140786	34.284314
1007.223294	67022.136492	34.289332
1008.758316	67114.431160	34.294349
1010.038566	67240.064321	34.299367
1010.949969	67351.347535	34.304384
1011.854423	67453.403074	34.309402
1012.443692	67562.944668	34.314420
1013.623278	67662.639118	34.319437
1014.323166	67784.963138	34.324455
1015.599897	67903.045670	34.329472
1016.922434	67994.986668	34.334490
1018.023988	68113.521612	34.339508
1019.125878	68218.588440	34.344525
1019.827374	68335.438450	34.349543
1021.083767	68439.944909	34.354560
1022.314963	68544.348541	34.359578
1023.069842	68650.768003	34.364596
1024.148371	68756.087836	34.369613
1025.087329	68859.762581	34.374631
1026.482240	68975.640602	34.379648
1027.381946	69077.035745	34.384666
1028.277074	69192.792394	34.389684
1029.607983	69295.111961	34.394701
1030.664640	69399.680612	34.399719
1031.476357	69505.937747	34.404736
1032.392791	69614.788090	34.409754
1033.576360	69718.624334	34.414772
1034.367180	69817.652463	34.419789
1035.679977	69931.451653	34.424807
1036.486912	70040.062738	34.429824
1037.780484	70137.306638	34.434842
1038.173657	70247.602114	34.439860
1039.770891	70333.331342	34.444877
1040.656746	70441.654098	34.449895
1041.451835	70539.844875	34.454912
1042.530662	70633.220752	34.459930
1043.492624	70734.387109	34.464948
1044.410278	70839.674237	34.469965
1045.058994	70952.694103	34.474983
1046.404623	71053.377739	34.480000
1047.739472	71164.855410	34.485018
1048.347679	71265.752211	34.490036
1049.484225	71377.426906	34.495053
1050.371666	71480.984688	34.500071
1051.322535	71613.263262	34.505088
1052.677260	71717.569361	34.510106
1053.605173	71826.575435	34.515124
1054.710323	71953.145002	34.520141
1055.764120	72065.468609	34.525159
1056.524177	72184.139333	34.530176
1057.906540	72297.328203	34.535194
1058.683387	72425.185160	34.540212
1059.954086	72540.137163	34.545229
1061.186089	72661.831896	34.550247
1062.194557	72775.563200	34.555264
1063.811354	72888.970909	34.560282
1064.593588	73013.052064	34.565300
1065.951370	73116.038047	34.570317
1066.642324	73238.163592	34.575335
1067.648268	73346.521051	34.580352
1069.054226	73463.080875	34.585370
1069.973643	73575.263767	34.590388
1071.432852	73689.048653	34.595405
1072.152146	73805.365824	34.600423
1073.336023	73921.679285	34.605440
1074.674626	74033.475790	34.610458
1075.524092	74144.794621	34.615476
1076.559180	74244.949822	34.620493
1077.742927	74370.795518	34.625511
1078.471540	74495.918147	34.630528
1079.940809	74606.357344	34.635546
1080.954559	74733.338261	34.640564
1082.018090	74833.112703	34.645581
1083.072891	74950.457472	34.650599
1083.951196	75085.538590	34.655616
1085.165255	75196.470318	34.660634
1086.626655	75315.243982	34.665652
1087.947373	75423.455166	34.670669
1088.654794	75542.463849	34.675687
1089.956015	75654.907304	34.680704
1091.087332	75769.533476	34.685722
1091.965708	75896.562216	34.690740
1093.411391	75994.151825	34.695757
1094.418452	76110.423912	34.700775
1095.139348	76220.200999	34.705792
1096.433414	76334.937210	34.710810
1097.443218	76439.057356	34.715828
1098.432119	76535.919585	34.720845
1099.053536	76653.671825	34.725863
1100.206323	76763.711808	34.730880
1101.468112	76863.148740	34.735898
1102.278558	76988.134745	34.740916
1103.458645	77092.092113	34.745933
1104.373383	77204.346511	34.750951
1105.557219	77324.288486	34.755968
1106.699190	77434.118928	34.760986
1107.632948	77561.484257	34.766004
1108.777175	77675.961137	34.771021
1109.573376	77806.535373	34.776039
1110.326696	77927.908273	34.781056
1112.092973	78038.951025	34.786074
1112.908698	78182.633377	34.791092
1114.199912	78305.686415	34.796109
1115.482878	78431.364583	34.801127
1116.119341	78565.407511	34.806144
1117.601053	78688.584250	34.811162
1118.421309	78821.133204	34.816180
1119.939075	78954.020857	34.821197
1121.187160	79078.855230	34.826215
1121.998357	79218.367462	34.831232
1123.469199	79341.429752	34.836250
1124.562638	79469.407319	34.841268
1125.639802	79596.092459	34.846285
1127.170061	79721.315683	34.851303
1127.821322	79867.659214	34.856320
1129.363831	79985.492720	34.861338
1130.414021	80106.123306	34.866356
1131.685733	80228.091070	34.871373
1132.905265	80370.403343	34.876391
1134.140479	80487.119151	34.881408
1135.660093	80608.227964	34.886426
1136.408395	80731.893880	34.891444
1137.824497	80848.500779	34.896461
1139.087939	80976.934752	34.901479
1140.046275	81100.834965	34.906496
1141.607276	81219.943182	34.911514
1142.360197	81350.888122	34.916532
1143.645290	81463.283866	34.921549
1144.792086	81579.330827	34.926567
1145.635957	81707.305022	34.931584
1147.001850	81821.617961	34.936602
1147.941166	81959.592105	34.941620
1149.197559	82072.893392	34.946637
1150.508043	82196.396424	34.951655
1151.279715	82340.449723	34.956672
1152.393130	82454.003403	34.961690
1153.867826	82574.252066	34.966708
1154.830017	82710.425778	34.971725
1155.871272	82841.220413	34.976743
1156.365514	82978.361684	34.981760
1157.951931	83084.630103	34.986778
1158.923050	83220.932150	34.991796
1160.079794	83323.363036	34.996813
1161.471975	83444.470661	35.001831
1162.556275	83569.503471	35.006848
1163.882875	83676.227149	35.011866
1164.629252	83801.846147	35.016884
1166.073443	83926.482443	35.021901
1166.987072	84043.617000	35.026919
1167.812742	84176.527960	35.031936
1169.334036	84291.392351	35.036954
1170.561533	84427.781563	35.041972
1171.582394	84558.141212	35.046989
1172.694729	84682.272039	35.052007
1174.025369	84812.109799	35.057024
1174.950896	84949.037230	35.062042
1176.260121	85079.815787	35.067060
1177.420699	85218.743485	35.072077
1178.592191	85339.296414	35.077095
1179.523113	85483.567158	35.082112
1180.911315	85609.802974	35.087130
1182.598805	85747.107566	35.092148
1183.974878	85884.348752	35.097165
1184.962555	86016.916688	35.102183
1186.136026	86140.148452	35.107200
1187.502556	86273.353268	35.112218
1188.394857	86414.392737	35.117236
1189.451162	86549.425389	35.122253
1191.070181	86681.783244	35.127271
1192.040052	86817.912594	35.132288
1193.263700	86953.679971	35.137306
1194.633888	87085.795347	35.142324
1196.162203	87224.544843	35.147341
1197.142986	87348.535066	35.152359
1198.347497	87479.351306	35.157376
1199.765458	87601.648364	35.162394
1200.765594	87739.043429	35.167412
1202.522309	87858.480465	35.172429
1203.931755	87990.658400	35.177447
1204.459209	88118.019705	35.182464
1206.023552	88241.960228	35.187482
1207.421053	88378.069403	35.192500
1208.284510	88516.022338	35.197517
1209.205730	88646.890713	35.202535
1210.431696	88776.933598	35.207552
1211.861596	88899.293033	35.212570
1212.936683	89045.158392	35.217588
1213.802517	89186.378326	35.222605
1215.279641	89314.582196	35.227623
1216.590112	89459.597128	35.232640
1217.661667	89587.367502	35.237658
1219.054200	89731.207582	35.242676
1220.112000	89866.241789	35.247693
1221.310605	89995.834670	35.252711
1222.351393	90134.402105	35.257728
1223.615290	90269.665333	35.262746
1224.783058	90394.680442	35.267764
1226.196709	90517.165407	35.272781
1227.395612	90645.162057	35.277799
1228.408278	90768.256077	35.282816
1229.791492	90889.894184	35.287834
1230.955083	91014.521390	35.292852
1232.156252	91150.293346	35.297869
1233.616846	91272.319716	35.302887
1234.539485	91407.524073	35.307904
1235.633908	91526.258074	35.312922
1237.169832	91660.443093	35.317940
1238.181806	91805.748739	35.322957
1239.644924	91931.484614	35.327975
1240.692269	92058.501658	35.332992
1241.947871	92183.108215	35.338010
1243.643729	92321.996432	35.343028
1244.764297	92456.935422	35.348045
1245.992031	92580.511383	35.353063
1247.452573	92727.617620	35.358080
1248.560979	92858.759727	35.363098
1249.464096	92997.107781	35.368116
1250.670479	93130.209313	35.373133
1251.806991	93264.606740	35.378151
1253.236159	93415.416371	35.383168
1253.977714	93567.772155	35.388186
1255.687799	93700.208784	35.393204
1256.569250	93862.803801	35.398221
1257.712856	94004.484917	35.403239
1259.115693	94158.162792	35.408256
1260.877583	94306.287907	35.413274
1262.170416	94453.400609	35.418292
1263.471124	94600.361218	35.423309
1264.597774	94748.027292	35.428327
1265.903975	94892.895215	35.433344
1267.208919	95048.353273	35.438362
1268.854844	95196.578632	35.443380
1269.940765	95334.235282	35.448397
1271.022406	95475.916593	35.453415
1272.214704	95636.874682	35.458432
1273.702524	95777.791165	35.463450
1274.939009	95930.641018	35.468468
1276.030851	96073.026632	35.473485
1277.824000	96218.104026	35.478503
1278.701260	96376.163287	35.483520
1280.143792	96515.870680	35.488538
1281.607318	96654.126941	35.493556
1282.670843	96804.226758	35.498573
1283.738818	96953.789143	35.503591
1285.300046	97101.926633	35.508608
1287.006817	97261.707439	35.513626
1288.245731	97400.560670	35.518644
1289.084290	97552.377650	35.523661
1290.760097	97694.155546	35.528679
1291.800648	97837.711795	35.533696
1293.173819	97993.603140	35.538714
1294.684541	98118.777852	35.543732
1295.738333	98263.992205	35.548749
1297.170039	98378.312040	35.553767
1298.099823	98515.203056	35.558784
1299.318224	98639.497095	35.563802
1300.482136	98781.983135	35.568820
1301.374468	98916.845339	35.573837
1302.981774	99062.989036	35.578855
1304.072716	99207.127931	35.583872
1305.069744	99362.322865	35.588890
1306.808846	99511.301840	35.593908
1307.963268	99655.275285	35.598925
1309.118672	99812.637171	35.603943
1310.227968	99971.772676	35.608960
1311.696779	100121.760264	35.613978
1313.019862	100271.537892	35.618996
1313.605144	100443.319076	35.624013
1315.349305	100600.295370	35.629031
1316.978305	100771.432219	35.634048
1317.944911	100925.212562	35.639066
1319.623537	101101.703097	35.644084
1320.829002	101259.547741	35.649101
1322.725971	101415.492902	35.654119
1323.941847	101581.139673	35.659136
1325.010319	101729.891542	35.664154
1326.405973	101893.778247	35.669172
1328.001592	102068.036735	35.674189
1329.480627	102218.339973	35.679207
1330.694169	102388.865061	35.684224
1332.114117	102544.526605	35.689242
1333.733770	102696.727840	35.694260
1334.970792	102863.943284	35.699277
1336.432442	103012.849635	35.704295
1337.789293	103177.517162	35.709312
1339.333761	103331.658122	35.714330
1340.594768	103485.535084	35.719348
1341.516321	103652.135524	35.724365
1343.136607	103798.610695	35.729383
1344.574892	103960.771210	35.734400
1346.149946	104121.341742	35.739418
1347.181925	104283.575383	35.744436
1348.784045	104436.632300	35.749453
1350.031084	104590.765485	35.754471
1351.084607	104753.233061	35.759488
1352.489008	104912.994435	35.764506
1354.138065	105066.263121	35.769524
1355.093623	105239.722888	35.774541
1356.625085	105395.942420	35.779559
1357.814929	105554.482857	35.784576
1359.276875	105718.221082	35.789594
1361.099436	105881.270263	35.794612
1362.400046	106039.903906	35.799629
1364.333358	106199.975892	35.804647
1365.391719	106354.068210	35.809664
1366.749688	106492.140289	35.814682
1368.323060	106629.058744	35.819700
1369.445061	106768.543253	35.824717
1370.754382	106910.397415	35.829735
1372.039950	107030.655888	35.834752
1373.391662	107177.080630	35.839770
1374.681201	107331.009570	35.844788
1375.729782	107458.554449	35.849805
1377.045807	107610.177229	35.854823
1378.473763	107761.960385	35.859840
1379.123005	107917.893542	35.864858
1380.840771	108062.999674	35.869876
1381.868169	108232.013965	35.874893
1383.463549	108389.774481	35.879911
1384.577220	108556.960851	35.884928
1385.928387	108727.344884	35.889946
1387.981768	108883.231978	35.894964
1389.082571	109048.297125	35.899981
1390.463511	109220.110314	35.904999
1391.824123	109388.674611	35.910016
1393.181786	109549.341343	35.915034
1395.108531	109701.506749	35.920052
1396.559906	109882.560847	35.925069
1397.778778	110042.328761	35.930087
1399.307467	110207.276773	35.935104
1400.336869	110377.837402	35.940122
1401.843037	110543.500181	35.945140
1403.238034	110722.119829	35.950157
1404.997686	110886.674904	35.955175
1406.751169	111041.408101	35.960192
1407.965297	111219.053650	35.965210
1408.993215	111376.486865	35.970228
1410.706642	111537.470878	35.975245
1412.559968	111715.164004	35.980263
1414.121500	111875.864190	35.985280
1415.480122	112027.399998	35.990298
1416.857299	112198.557287	35.995316
1417.994049	112360.992958	36.000333
1419.864687	112524.395535	36.005351
1421.084879	112692.435042	36.010368
1422.558063	112858.270504	36.015386
1424.314990	113016.218646	36.020404
1425.240973	113177.110542	36.025421
1426.666499	113340.867751	36.030439
1427.862726	113512.480635	36.035456
1429.361271	113677.817402	36.040474
1430.710088	113835.170869	36.045492
1432.335921	114017.164400	36.050509
1434.026396	114177.472769	36.055527
1435.343872	114348.926504	36.060544
1436.656175	114517.704322	36.065562
1438.315261	114675.463231	36.070580
1439.511189	114847.705704	36.075597
1440.894487	115016.203351	36.080615
1442.821044	115182.792491	36.085632
1444.085809	115343.150603	36.090650
1445.301610	115495.287216	36.095668
1446.355537	115646.652754	36.100685
1447.528261	115799.633735	36.105703
1449.138843	115956.730923	36.110720
1450.434472	116128.687694	36.115738
1452.145591	116273.589729	36.120756
1453.215703	116448.249926	36.125773
1454.748048	116614.290647	36.130791
1456.043936	116780.370022	36.135808
1457.786825	116945.436076	36.140826
1459.311724	117104.250759	36.145844
1460.478737	117293.349581	36.150861
1461.893411	117458.680036	36.155879
1463.517541	117632.728441	36.160896
1464.756422	117801.641025	36.165914
1466.084055	117973.092254	36.170932
1467.481173	118163.883115	36.175949
1469.073539	118335.959517	36.180967
1470.714048	118516.950841	36.185984
1472.035746	118698.114395	36.191002
1473.376214	118880.618582	36.196020
1475.149918	119076.238185	36.201037
1476.584695	119259.724163	36.206055
1478.142614	119446.357855	36.211072
1479.699782	119629.200130	36.216090
1481.242753	119802.585854	36.221108
1482.837179	119995.372442	36.226125
1484.534666	120185.788521	36.231143
1486.036963	120370.056781	36.236160
1487.319787	120544.660226	36.241178
1489.322507	120732.726857	36.246196
1490.856580	120919.159574	36.251213
1492.026600	121096.114911	36.256231
1493.888575	121277.444844	36.261248
1495.185395	121450.190361	36.266266
1496.668307	121621.868915	36.271284
1498.300004	121812.433904	36.276301
1499.410052	121998.523690	36.281319
1501.001182	122177.445805	36.286336
1502.489195	122370.646690	36.291354
1503.917380	122559.653565	36.296372
1505.424399	122748.915236	36.301389
1507.082433	122932.619388	36.306407
1508.828191	123109.319407	36.311424
1510.431801	123288.740995	36.316442
1512.252755	123471.257729	36.321460
1514.087136	123648.352551	36.326477
1515.404085	123823.795509	36.331495
1516.971205	123992.284171	36.336512
1518.573121	124173.814550	36.341530
1519.984057	124342.735548	36.346548
1521.455605	124530.229537	36.351565
1522.942172	124706.157975	36.356583
1524.777758	124872.367548	36.361600
1525.962635	125056.465452	36.366618
1527.554318	125198.484562	36.371636
1528.738905	125366.941281	36.376653
1530.372621	125522.850860	36.381671
1531.451692	125690.591682	36.386688
1533.202092	125856.440841	36.391706
1534.683030	126019.407732	36.396724
1536.253975	126181.233927	36.401741
1537.628493	126359.749688	36.406759
1539.221527	126528.478079	36.411776
1540.294220	126706.005341	36.416794
1541.733462	126877.078454	36.421812
1543.460694	127055.922762	36.426829
1544.760606	127242.158018	36.431847
1546.263281	127433.809449	36.436864
1547.942779	127617.466076	36.441882
1549.266104	127796.214704	36.446900
1550.675742	127986.250613	36.451917
1552.094407	128188.688437	36.456935
1554.120983	128373.219744	36.461952
1555.357810	128577.678211	36.466970
1557.152331	128765.276715	36.471988
1558.754638	128963.763864	36.477005
1560.157199	129165.932699	36.482023
1562.047461	129350.010777	36.487040
1563.660720	129546.891447	36.492058
1565.500052	129746.803441	36.497076
1566.844853	129946.035298	36.502093
1568.324421	130145.817272	36.507111
1570.463129	130332.700228	36.512128
1571.556488	130531.456771	36.517146
1573.147449	130720.747783	36.522164
1574.871076	130929.301688	36.527181
1576.248047	131122.138800	36.532199
1577.950210	131316.129177	36.537216
1579.612427	131518.565175	36.542234
1581.596379	131711.905376	36.547252
1583.043778	131907.967442	36.552269
1584.525494	132102.935808	36.557287
1586.454625	132300.659840	36.562304
1588.116360	132505.244196	36.567322
1589.699630	132694.727052	36.572340
1591.403924	132883.292362	36.577357
1592.941354	133079.626965	36.582375
1594.891376	133276.302832	36.587392
1596.292648	133467.416201	36.592410
1598.022100	133647.163936	36.597428
1599.526485	133842.812152	36.602445
1600.785524	134035.434366	36.607463
1603.097841	134216.398169	36.612480
1604.582659	134412.002689	36.617498
1606.350156	134599.441561	36.622516
1608.104035	134785.211239	36.627533
1609.346250	134971.810981	36.632551
1611.593173	135155.287282	36.637568
1612.681276	135332.182356	36.642586
1614.543009	135486.856814	36.647604
1615.994156	135651.772451	36.652621
1617.374032	135827.889261	36.657639
1618.979356	135985.774976	36.662656
1620.456795	136152.513980	36.667674
1621.805946	136326.851990	36.672692
1623.530356	136496.164102	36.677709
1624.791301	136681.314589	36.682727
1626.850144	136852.273673	36.687744
1628.164040	137024.277134	36.692762
1629.985298	137205.869812	36.697780
1631.599880	137381.629233	36.702797
1632.793349	137569.837359	36.707815
1634.910479	137743.301480	36.712832
1636.247536	137941.791764	36.717850
1637.682898	138126.049249	36.722868
1639.584241	138312.514931	36.727885
1640.872401	138511.308271	36.732903
1642.792644	138706.454188	36.737920
1644.201153	138902.341651	36.742938
1645.977701	139095.548661	36.747956
1647.504830	139299.847369	36.752973
1648.793796	139506.859317	36.757991
1650.461010	139694.498752	36.763008
1651.924672	139910.623082	36.768026
1653.751874	140119.125260	36.773044
1655.660299	140335.587560	36.778061
1657.309912	140541.966398	36.783079
1659.781927	140721.550830	36.788096
1661.021644	140942.546775	36.793114
1662.574452	141151.682671	36.798132
1664.715646	141338.496661	36.803149
1666.379508	141555.133290	36.808167
1668.307052	141751.615940	36.813184
1669.916268	141959.240241	36.818202
1671.202347	142160.440775	36.823220
1673.164855	142362.422408	36.828237
1674.733528	142570.729048	36.833255
1676.570446	142759.437870	36.838272
1678.177515	142975.447215	36.843290
1679.706367	143162.851273	36.848308
1681.759170	143361.719886	36.853325
1683.205391	143568.214920	36.858343
1685.150227	143768.700329	36.863360
1686.534891	143982.838165	36.868378
1688.506175	144184.931792	36.873396
1690.201084	144391.659011	36.878413
1691.649868	144602.495425	36.883431
1693.075693	144805.300801	36.888448
1694.770672	145005.808545	36.893466
1696.729486	145214.578083	36.898484
1698.655907	145420.933141	36.903501
1700.033509	145633.587756	36.908519
1701.939293	145839.619288	36.913536
1703.526495	146032.215759	36.918554
1705.330407	146229.354974	36.923572
1707.019494	146414.826468	36.928589
1708.690484	146602.292059	36.933607
1710.194732	146784.702143	36.938624
1711.827582	146966.674546	36.943642
1713.249537	147160.178804	36.948660
1715.031852	147351.750929	36.953677
1716.609854	147559.164079	36.958695
1718.517895	147754.090581	36.963712
1720.256434	147956.207428	36.968730
1721.725210	148157.797946	36.973748
1723.415920	148355.437399	36.978765
1725.322213	148560.003383	36.983783
1727.174200	148758.697243	36.988800
1728.354898	148979.506067	36.993818
1730.043077	149176.770677	36.998836
1731.922476	149396.153003	37.003853
1733.566966	149612.480892	37.008871
1735.129503	149825.058096	37.013888
1737.072595	150049.302812	37.018906
1739.061739	150253.511426	37.023924
1740.946301	150470.871831	37.028941
1742.605058	150685.024077	37.033959
1744.649015	150897.633280	37.038976
1746.478873	151120.356683	37.043994
1748.168214	151338.603278	37.049012
1750.355208	151547.707589	37.054029
1751.886696	151766.032805	37.059047
1753.651668	151977.894602	37.064064
1755.576766	152173.314106	37.069082
1757.121147	152388.978987	37.074100
1758.996051	152611.451775	37.079117
1760.677850	152819.642784	37.084135
1762.516903	153034.390272	37.089152
1764.564343	153265.829111	37.094170
1766.132143	153480.356297	37.099188
1768.079290	153682.424817	37.104205
1769.662634	153902.049100	37.109223
1771.585254	154113.405023	37.114240
1773.354719	154325.724841	37.119258
1775.664957	154563.128099	37.124276
1777.523358	154748.899175	37.129293
1779.202600	154963.215289	37.134311
1781.051169	155166.449526	37.139328
1783.011425	155371.378968	37.144346
1784.645304	155583.702875	37.149364
1786.420524	155779.509595	37.154381
1788.116868	155996.682427	37.159399
1789.960454	156222.582255	37.164416
1791.627912	156413.997199	37.169434
1793.443069	156625.880390	37.174452
1795.582552	156842.303534	37.179469
1797.165905	157050.029095	37.184487
1798.810186	157246.258089	37.189504
1801.135730	157443.166213	37.194522
1802.399270	157643.984732	37.199540
1804.282421	157831.391744	37.204557
1805.821845	158028.161724	37.209575
1807.822220	158210.809727	37.214592
1809.496083	158404.694725	37.219610
1810.977490	158590.026615	37.224628
1812.436705	158787.878800	37.229645
1814.186584	158987.879726	37.234663
1815.915373	159198.118537	37.239680
1817.883761	159414.559558	37.244698
1819.341174	159621.483563	37.249716
1821.311102	159823.242337	37.254733
1822.763943	160043.991858	37.259751
1824.233658	160271.524506	37.264768
1826.486385	160493.075577	37.269786
1828.160235	160728.390408	37.274804
1830.280277	160942.229739	37.279821
1832.050069	161168.388959	37.284839
1833.937439	161383.650163	37.289856
1835.906503	161618.150438	37.294874
1837.986099	161851.823075	37.299892
1839.802907	162070.942184	37.304909
1841.965678	162299.290855	37.309927
1843.480337	162529.329106	37.314944
1845.553781	162752.622044	37.319962
1846.943034	162980.019844	37.324980
1848.613737	163212.447277	37.329997
1850.611317	163440.778659	37.335015
1852.577230	163670.511564	37.340032
1854.475913	163925.063471	37.345050
1856.449583	164157.436165	37.350068
1858.592753	164381.108517	37.355085
1860.554150	164616.009911	37.360103
1862.520236	164853.803735	37.365120
1864.690863	165079.555961	37.370138
1866.155064	165307.514387	37.375156
1868.224159	165524.293250	37.380173
1870.306740	165764.839347	37.385191
1872.334335	165990.505688	37.390208
1874.473039	166217.005541	37.395226
1875.961100	166442.570015	37.400244
1878.002740	166667.616745	37.405261
1880.218483	166884.494404	37.410279
1882.163700	167107.745348	37.415296
1884.133647	167327.150556	37.420314
1886.099310	167541.281306	37.425332
1888.285052	167761.542650	37.430349
1890.127187	167989.432070	37.435367
1892.255799	168190.641171	37.440384
1894.002254	168398.165197	37.445402
1895.640743	168616.945560	37.450420
1897.639318	168822.529275	37.455437
1899.449718	169047.715671	37.460455
1901.359361	169268.727200	37.465472
1903.676298	169477.815501	37.470490
1905.175731	169668.654997	37.475508
1907.083869	169852.898074	37.480525
1908.715411	170047.637977	37.485543
1910.215506	170236.323808	37.490560
1912.656561	170423.047309	37.495578
1913.930528	170628.501991	37.500596
1915.683274	170824.469664	37.505613
1917.604868	171034.593180	37.510631
1919.337636	171242.870430	37.515648
1921.481104	171451.552951	37.520666
1922.949329	171666.990719	37.525684
1925.142748	171874.107302	37.530701
1926.732265	172105.511472	37.535719
1928.506613	172318.164220	37.540736
1930.683247	172535.929880	37.545754
1932.368886	172770.481337	37.550772
1934.567417	172990.630878	37.555789
1936.712029	173218.503008	37.560807
1938.436765	173450.553218	37.565824
1940.584511	173681.243702	37.570842
1942.137347	173907.564541	37.575860
1944.563922	174128.978117	37.580877
1946.297163	174363.861206	37.585895
1948.411461	174595.665926	37.590912
1950.599595	174827.637863	37.595930
1952.719657	175063.884472	37.600948
1954.791487	175288.646415	37.605965
1956.942159	175509.109131	37.610983
1958.854113	175746.001669	37.616000
1960.949585	175969.317372	37.621018
1963.124615	176201.565634	37.626036
1965.126446	176434.337473	37.631053
1967.238324	176657.844617	37.636071
1968.680082	176884.973529	37.641088
1971.213359	177107.274433	37.646106
1972.997438	177332.905189	37.651124
1974.796390	177550.973422	37.656141
1977.058363	177780.666698	37.661159
1978.755086	178009.347166	37.666176
1981.128238	178231.248129	37.671194
1983.108433	178456.790407	37.676212
1985.177468	178693.395754	37.681229
1987.202371	178913.528624	37.686247
1989.071489	179140.728853	37.691264
1991.224472	179352.977518	37.696282
1993.052471	179582.825630	37.701300
1995.455048	179796.648222	37.706317
1997.417859	180024.599568	37.711335
1999.199653	180246.795263	37.716352
2001.290241	180467.331765	37.721370
2003.166000	180688.525194	37.726388
2005.523775	180903.921034	37.731405
2007.541422	181128.697573	37.736423
2009.365587	181345.423710	37.741440
2011.854882	181550.943318	37.746458
2013.525321	181747.965895	37.751476
2015.258917	181960.129055	37.756493
2017.511963	182143.446539	37.761511
2019.477616	182334.626395	37.766528
2021.357727	182526.607338	37.771546
2023.434711	182715.398467	37.776564
2025.392705	182906.493214	37.781581
2027.413464	183119.568061	37.786599
2029.316076	183306.270407	37.791616
2031.280831	183504.066247	37.796634
2033.372455	183720.723635	37.801652
2035.230709	183909.402311	37.806669
2037.560499	184120.783402	37.811687
2039.454480	184338.845551	37.816704
2041.643887	184541.406755	37.821722
2043.416264	184760.771836	37.826740
2045.184837	184966.015663	37.831757
2047.864940	185189.806876	37.836775
2049.273033	185399.652577	37.841792
2051.965406	185604.359372	37.846810
2054.008971	185830.843356	37.851828
2056.126268	186029.095629	37.856845
2058.240050	186243.934388	37.861863
2060.159005	186452.650673	37.866880
2062.382881	186670.773234	37.871898
2064.149228	186898.473930	37.876916
2066.851100	187111.053529	37.881933
2069.453733	187322.761575	37.886951
2071.049575	187543.678129	37.891968
2073.419590	187752.392190	37.896986
2075.094713	187964.732533	37.902004
2077.165010	188174.320880	37.907021
2079.572904	188392.447742	37.912039
2081.499945	188610.575767	37.917056
2083.730736	188809.443774	37.922074
2085.916514	189040.451288	37.927092
2087.644784	189257.217925	37.932109
2090.346746	189452.346418	37.937127
2092.478296	189693.441817	37.942144
2094.888645	189878.389902	37.947162
2096.655148	190099.075653	37.952180
2098.871707	190304.335497	37.957197
2100.989895	190510.462097	37.962215
2103.196071	190714.126333	37.967232
2105.831424	190920.972162	37.972250
2107.706851	191130.706012	37.977268
2109.545650	191336.804327	37.982285
2111.882756	191528.559965	37.987303
2113.588826	191742.752432	37.992320
2115.808865	191943.805323	37.997338
2117.981171	192160.552690	38.002356
2120.175614	192368.109181	38.007373
2122.108028	192564.083062	38.012391
2124.241400	192780.179406	38.017408
2126.809806	192965.139600	38.022426
2129.052767	193156.104313	38.027444
2130.733463	193336.828231	38.032461
2133.072328	193504.693600	38.037479
2134.762523	193683.564337	38.042496
2137.030831	193860.630668	38.047514
2139.074609	194046.503058	38.052532
2140.936946	194235.692026	38.057549
2142.848871	194425.178439	38.062567
2144.772249	194616.669026	38.067584
2146.897516	194806.986065	38.072602
2148.580856	195031.413131	38.077620
2150.608774	195242.840911	38.082637
2152.984953	195433.843937	38.087655
2154.916595	195663.514208	38.092672
2157.095730	195879.020121	38.097690
2158.938195	196091.864256	38.102708
2161.075391	196318.052632	38.107725
2163.516906	196534.979265	38.112743
2165.219832	196779.299408	38.117760
2167.706592	197000.079232	38.122778
2169.540920	197223.616162	38.127796
2171.919324	197453.528147	38.132813
2174.088163	197696.915615	38.137831
2176.267691	197933.512061	38.142848
2178.878167	198157.869113	38.147866
2180.926807	198410.925245	38.152884
2183.480703	198638.263371	38.157901
2185.819969	198861.181387	38.162919
2188.045877	199103.220857	38.167936
2190.305214	199326.458121	38.172954
2192.971449	199555.889343	38.177972
2194.914729	199776.335414	38.182989
2197.362879	200015.970184	38.188007
2199.627764	200242.891321	38.193024
2201.941949	200461.872439	38.198042
2204.327606	200687.938541	38.203060
2206.515593	200911.879097	38.208077
2208.844573	201128.575779	38.213095
2211.075442	201356.852424	38.218112
2212.900364	201581.259475	38.223130
2215.240506	201806.778900	38.228148
2217.424450	202034.012237	38.233165
2219.939650	202262.476008	38.238183
2221.511474	202499.011075	38.243200
2223.937102	202718.681626	38.248218
2226.207543	202953.483041	38.253236
2228.381036	203194.964984	38.258253
2230.451437	203421.879229	38.263271
2232.600200	203662.910117	38.268288
2235.096430	203892.513260	38.273306
2237.345911	204128.198741	38.278324
2239.452280	204361.940331	38.283341
2241.850439	204596.931384	38.288359
2244.363145	204840.499087	38.293376
2246.146319	205055.939185	38.298394
2248.599587	205271.223043	38.303412
2250.378448	205483.936176	38.308429
2252.336660	205693.689280	38.313447
2254.358515	205909.323179	38.318464
2256.544730	206116.045794	38.323482
2258.777729	206348.594720	38.328500
2260.627853	206580.760973	38.333517
2262.802974	206811.937208	38.338535
2264.815548	207056.228150	38.343552
2266.800366	207281.508050	38.348570
2269.234656	207530.507208	38.353588
2271.530793	207786.219390	38.358605
2274.106965	208021.195872	38.363623
2276.283625	208282.819444	38.368640
2278.454496	208517.100431	38.373658
2281.080915	208774.694018	38.378676
2283.074115	209028.199774	38.383693
2285.802879	209272.449561	38.388711
2288.343986	209536.661253	38.393728
2290.655508	209785.803338	38.398746
2292.829092	210026.322916	38.403764
2294.784725	210300.228197	38.408781
2297.419379	210532.754825	38.413799
2299.506876	210810.945103	38.418816
2302.388971	211059.189282	38.423834
2304.690867	211325.173006	38.428852
2306.874300	211569.848299	38.433869
2309.433048	211829.801158	38.438887
2311.472309	212092.173416	38.443904
2313.818303	212345.865110	38.448922
2316.437661	212605.900358	38.453940
2318.448076	212873.472868	38.458957
2321.406496	213132.732806	38.463975
2323.298829	213400.288104	38.468992
2325.614092	213653.456529	38.474010
2328.073772	213913.725417	38.479028
2330.225522	214185.800582	38.484045
2332.532561	214441.639462	38.489063
2335.067791	214703.689588	38.494080
2337.537932	214973.965422	38.499098
2339.685866	215241.462183	38.504116
2342.023093	215516.712748	38.509133
2344.597612	215775.053505	38.514151
2346.605133	216046.448036	38.519168
2349.200883	216317.686895	38.524186
2352.159026	216572.821140	38.529204
2354.448348	216844.250303	38.534221
2356.756141	217105.228394	38.539239
2359.230378	217363.070420	38.544256
2361.306925	217641.938480	38.549274
2363.917815	217900.674960	38.554292
2366.206857	218158.498462	38.559309
2368.909488	218405.071526	38.564327
2370.994322	218672.248638	38.569344
2373.187122	218927.550813	38.574362
2375.479124	219155.552646	38.579380
2377.498636	219397.044391	38.584397
2380.079541	219626.817557	38.589415
2382.205666	219867.913049	38.594432
2384.475043	220112.338631	38.599450
2386.527760	220351.796732	38.604468
2388.774882	220604.467850	38.609485
2391.467265	220869.156911	38.614503
2393.612877	221123.458411	38.619520
2395.799353	221379.569995	38.624538
2397.895509	221652.114326	38.629556
2400.015206	221910.892018	38.634573
2402.089452	222179.911857	38.639591
2404.757704	222457.866326	38.644608
2407.154048	222750.238406	38.649626
2409.619313	223028.773093	38.654644
2411.800600	223325.003366	38.659661
2414.268129	223602.117609	38.664679
2416.681891	223905.830187	38.669696
2418.857383	224188.554338	38.674714
2421.945153	224539.385167	38.679732
2424.069781	224838.753705	38.684749
2426.497475	225136.627759	38.689767
2428.997604	225434.085090	38.694784
2431.495943	225736.826120	38.699802
2434.084594	226031.427251	38.704820
2436.757347	226339.793439	38.709837
2439.447878	226619.434949	38.714855
2442.002451	226923.453894	38.719872
2444.675439	227219.226767	38.724890
2446.999012	227514.979865	38.729908
2449.768163	227805.711053	38.734925
2452.172549	228094.062972	38.739943
2455.041055	228387.421615	38.744960
2457.352004	228683.231516	38.749978
2460.091524	228971.736400	38.754996
2462.592563	229267.568933	38.760013
2465.094758	229544.862484	38.765031
2467.415640	229847.760460	38.770048
2469.962406	230133.861549	38.775066
2472.822919	230414.326431	38.780084
2475.298577	230716.517063	38.785101
2477.731512	230999.819818	38.790119
2479.871763	231278.826869	38.795136
2482.253236	231572.781066	38.800154
2484.575804	231876.726783	38.805172
2487.235401	232174.778599	38.810189
2489.826036	232471.216826	38.815207
2492.164111	232756.876521	38.820224
2494.517196	233064.834061	38.825242
2497.086739	233351.601742	38.830260
2499.329746	233662.194616	38.835277
2502.111640	233959.699213	38.840295
2504.791493	234254.477871	38.845312
2507.130199	234551.470322	38.850330
2509.638000	234820.346252	38.855348
2511.728841	235093.200337	38.860365
2514.539306	235356.569063	38.865383
2516.578642	235637.611087	38.870400
2519.046054	235916.731937	38.875418
2521.360358	236184.245193	38.880436
2523.577729	236463.737319	38.885453
2525.694686	236757.977430	38.890471
2528.462937	237048.279909	38.895488
2531.184693	237344.762500	38.900506
2533.560635	237643.561225	38.905524
2535.888771	237949.251512	38.910541
2538.475268	238245.961193	38.915559
2540.889788	238557.125708	38.920576
2543.294099	238861.333294	38.925594
2545.991743	239167.958963	38.930612
2548.304772	239480.640687	38.935629
2551.116845	239807.772727	38.940647
2554.006631	240120.364803	38.945664
2556.341438	240444.018325	38.950682
2559.052017	240759.586874	38.955700
2561.359571	241088.428033	38.960717
2564.746204	241397.287197	38.965735
2567.335660	241719.151247	38.970752
2569.710515	242036.249548	38.975770
2572.516168	242348.200390	38.980788
2575.022780	242669.572054	38.985805
2577.641538	242989.859964	38.990823
2580.537560	243308.910939	38.995840
2582.952798	243630.832929	39.000858
2585.574372	243943.350279	39.005876
2588.051104	244272.884238	39.010893
2590.652632	244596.557125	39.015911
2593.824577	244911.809028	39.020928
2596.087806	245243.766872	39.025946
2599.098545	245564.049765	39.030964
2601.573232	245888.330056	39.035981
2603.971013	246214.807759	39.040999
2606.984746	246531.460090	39.046016
2609.428741	246856.839715	39.051034
2612.087894	247171.390564	39.056052
2614.581335	247508.905496	39.061069
2617.561265	247828.385542	39.066087
2620.542641	248152.031835	39.071104
2622.650845	248478.890710	39.076122
2625.508266	248789.196964	39.081140
2628.124475	249114.300225	39.086157
2630.688598	249436.491256	39.091175
2633.631429	249765.227314	39.096192
2635.984796	250079.883413	39.101210
2638.676908	250409.117732	39.106228
2640.908740	250728.595222	39.111245
2643.925650	251053.003870	39.116263
2646.566500	251381.994217	39.121280
2649.104524	251714.278308	39.126298
2651.443736	251998.915421	39.131316
2653.883589	252300.607062	39.136333
2656.609047	252602.406380	39.141351
2659.239266	252902.874991	39.146368
2661.504997	253205.942031	39.151386
2664.238930	253497.021871	39.156404
2666.583654	253819.382890	39.161421
2668.863392	254130.196814	39.166439
2671.616924	254453.738836	39.171456
2673.607397	254780.780753	39.176474
2676.510133	255106.713409	39.181492
2679.026938	255443.910103	39.186509
2681.713253	255789.564850	39.191527
2684.404297	256143.779992	39.196544
2686.493405	256484.323001	39.201562
2689.561209	256833.957976	39.206580
2691.916285	257192.648056	39.211597
2694.513863	257558.692406	39.216615
2697.480641	257920.309621	39.221632
2700.270758	258288.204399	39.226650
2702.922598	258658.001433	39.231668
2705.611355	259037.014322	39.236685
2708.680210	259397.017194	39.241703
2711.304310	259775.330146	39.246720
2713.979368	260147.843747	39.251738
2716.939964	260515.765537	39.256756
2719.568516	260888.846369	39.261773
2722.438686	261266.334913	39.266791
2725.500549	261639.424289	39.271808
2728.386127	262024.430602	39.276826
2731.250029	262387.314885	39.281844
2734.121242	262766.126071	39.286861
2737.018804	263133.273555	39.291879
2739.779784	263494.701992	39.296896
2742.386094	263867.789888	39.301914
2745.506288	264235.208107	39.306932
2748.363372	264606.504227	39.311949
2750.842330	264985.075073	39.316967
2754.123689	265348.937799	39.321984
2756.726197	265723.857117	39.327002
2759.521810	266099.178032	39.332020
2762.236746	266471.031801	39.337037
2764.809436	266833.178965	39.342055
2768.205746	267206.805230	39.347072
2770.580706	267590.195952	39.352090
2773.064212	267955.660457	39.357108
2776.347276	268323.437284	39.362125
2778.833671	268704.728045	39.367143
2781.774602	269081.577683	39.372160
2784.466798	269456.688693	39.377178
2787.451914	269827.511154	39.382196
2790.188466	270201.955033	39.387213
2792.972897	270569.049930	39.392231
2795.670074	270942.611253	39.397248
2798.218116	271316.221742	39.402266
2801.067656	271649.418640	39.407284
2803.574517	271994.812724	39.412301
2806.171960	272343.901451	39.417319
2808.830293	272697.858074	39.422336
2811.636829	273039.597670	39.427354
2814.404266	273400.599304	39.432372
2816.828939	273759.470581	39.437389
2819.598410	274121.945394	39.442407
2822.403207	274484.211420	39.447424
2824.691154	274862.004592	39.452442
2827.859129	275235.847908	39.457460
2830.451520	275620.273979	39.462477
2832.824432	276001.686379	39.467495
2835.818955	276377.513179	39.472512
2838.851695	276776.323974	39.477530
2841.393561	277174.399526	39.482548
2844.468097	277572.085814	39.487565
2847.341453	277974.097038	39.492583
2850.273148	278366.725065	39.497600
2852.924486	278791.558040	39.502618
2855.972772	279189.984709	39.507636
2858.984081	279603.836915	39.512653
2861.512523	280015.987158	39.517671
2864.831682	280417.698245	39.522688
2867.645915	280834.832679	39.527706
2870.602393	281249.505631	39.532724
2873.553565	281666.059011	39.537741
2876.175333	282081.952979	39.542759
2879.354336	282503.042301	39.547776
2882.459891	282930.925596	39.552794
2885.454659	283343.863595	39.557812
2888.771244	283768.588184	39.562829
2891.241839	284179.093550	39.567847
2894.392998	284593.453683	39.572864
2897.418143	285009.662395	39.577882
2900.930747	285415.403650	39.582900
2903.980392	285828.559274	39.587917
2906.924531	286235.024756	39.592935
2910.082491	286633.403186	39.597952
2912.779869	287056.825214	39.602970
2916.023827	287457.958014	39.607988
2919.267084	287861.529120	39.613005
2921.813832	288265.972075	39.618023
2924.634910	288662.140552	39.623040
2927.676800	289070.365291	39.628058
2930.420913	289483.082091	39.633076
2933.599354	289895.805742	39.638093
2936.200070	290307.908963	39.643111
2939.441557	290704.287477	39.648128
2942.512404	291119.312530	39.653146
2944.954648	291534.284005	39.658164
2948.256960	291945.384463	39.663181
2951.063133	292358.137723	39.668199
2953.886214	292769.185624	39.673216
2956.488437	293163.349757	39.678234
2959.378681	293554.927375	39.683252
2962.179245	293937.068837	39.688269
2964.754970	294311.472124	39.693287
2967.594059	294696.222574	39.698304
2970.120758	295107.465431	39.703322
2972.741253	295498.904359	39.708340
2975.901191	295893.000557	39.713357
2978.641478	296310.608460	39.718375
2981.504642	296715.774448	39.723392
2984.308502	297134.411969	39.728410
2987.260336	297552.745702	39.733428
2990.092732	297982.883813	39.738445
2992.768914	298419.726270	39.743463
2996.052191	298851.518219	39.748480
2998.592741	299295.314598	39.753498
3001.982189	299747.662768	39.758516
3004.947832	300195.860143	39.763533
3007.798813	300657.384763	39.768551
3010.768982	301095.799390	39.773568
3013.814315	301562.142266	39.778586
3016.988937	302012.663747	39.783604
3020.122924	302479.726433	39.788621
3023.349055	302943.369338	39.793639
3026.921189	303394.585765	39.798656
3029.386023	303862.511991	39.803674
3032.659785	304327.717768	39.808692
3036.008799	304795.678761	39.813709
3039.240796	305260.456209	39.818727
3042.216977	305715.975968	39.823744
3045.258258	306201.532557	39.828762
3048.569519	306660.094887	39.833780
3051.748410	307124.289993	39.838797
3054.624497	307587.032725	39.843815
3057.819774	308051.094842	39.848832
3061.072723	308524.493275	39.853850
3064.327298	308993.673244	39.858868
3067.763572	309452.383335	39.863885
3070.272624	309915.403940	39.868903
3073.367633	310386.457842	39.873920
3076.848297	310861.715902	39.878938
3080.257920	311324.308959	39.883956
3083.654003	311778.698309	39.888973
3086.528334	312252.116123	39.893991
3089.604246	312703.148863	39.899008
3092.161964	313173.412514	39.904026
3095.378257	313645.347801	39.909044
3098.648694	314105.639821	39.914061
3101.988295	314578.592761	39.919079
3105.082391	315041.549999	39.924096
3108.108493	315506.623963	39.929114
3111.180493	315973.796577	39.934132
3114.439072	316429.457539	39.939149
3117.371953	316919.404420	39.944167
3120.694591	317373.628580	39.949184
3123.574028	317833.076476	39.954202
3126.128302	318271.976147	39.959220
3129.762385	318700.848687	39.964237
3132.435638	319129.109377	39.969255
3135.012814	319563.707212	39.974272
3138.037073	320010.702247	39.979290
3141.144014	320450.520042	39.984308
3144.227572	320900.777513	39.989325
3147.269291	321358.683756	39.994343
3150.597186	321810.523341	39.999360
3153.688400	322272.124898	40.004378
3156.248395	322732.792191	40.009396
3159.498466	323214.401289	40.014413
3162.551505	323673.918846	40.019431
3165.832673	324156.990620	40.024448
3168.660708	324641.908990	40.029466
3171.972649	325123.167159	40.034484
3175.159935	325609.495914	40.039501
3178.423529	326118.436904	40.044519
3181.267703	326612.610240	40.049536
3184.492223	327101.895268	40.054554
3187.702672	327618.275769	40.059572
3190.773923	328117.787405	40.064589
3193.835976	328645.789889	40.069607
3197.435791	329143.306628	40.074624
3201.033052	329664.310091	40.079642
3204.110021	330173.863371	40.084660
3207.574110	330680.304646	40.089677
3210.730074	331208.553514	40.094695
3214.139892	331712.101352	40.099712
3217.626306	332235.998954	40.104730
3220.744216	332745.680100	40.109748
3224.013539	333264.068780	40.114765
3227.231357	333790.917547	40.119783
3231.000111	334304.572630	40.124800
3234.079931	334823.487512	40.129818
3237.179958	335342.674569	40.134836
3240.902722	335858.001128	40.139853
3243.992813	336381.193687	40.144871
3247.105422	336901.788635	40.149888
3250.500467	337421.674625	40.154906
3253.963501	337948.604467	40.159924
3257.531695	338448.878312	40.164941
3260.968368	338972.071514	40.169959
3264.347686	339485.570325	40.174976
3267.033134	339995.823209	40.179994
3270.580188	340511.724607	40.185012
3274.085983	341029.354776	40.190029
3277.351395	341550.750920	40.195047
3280.695622	342064.056319	40.200064
3284.091134	342583.975875	40.205082
3287.322069	343102.088979	40.210100
3290.496654	343603.297569	40.215117
3294.321860	344127.248771	40.220135
3297.449976	344636.301056	40.225152
3300.681313	345132.333861	40.230170
3303.910155	345612.165326	40.235188
3306.854958	346082.009577	40.240205
3309.732557	346544.447454	40.245223
3312.615588	347028.916925	40.250240
3315.859682	347498.042110	40.255258
3318.673013	347994.700135	40.260276
3321.826285	348482.897000	40.265293
3324.879689	348986.159527	40.270311
3328.415354	349494.748453	40.275328
3331.367626	349992.483574	40.280346
3334.464514	350532.026946	40.285364
3338.282949	351033.042603	40.290381
3341.447024	351567.208645	40.295399
3344.841257	352097.829809	40.300416
3348.265470	352613.337007	40.305434
3351.346471	353151.815603	40.310452
3355.063808	353687.344983	40.315469
3358.641344	354223.652461	40.320487
3361.829995	354756.563675	40.325504
3364.885683	355303.730457	40.330522
3368.272465	355857.286303	40.335540
3372.249316	356392.010220	40.340557
3375.306944	356947.941338	40.345575
3379.151194	357485.872721	40.350592
3382.273175	358041.375297	40.355610
3385.409578	358594.635721	40.360628
3389.281385	359154.778858	40.365645
3392.568923	359729.551305	40.370663
3396.053656	360279.184064	40.375680
3399.755572	360841.948667	40.380698
3402.933557	361403.926525	40.385716
3406.554010	361973.467089	40.390733
3410.094395	362532.430093	40.395751
3413.365367	363102.951204	40.400768
3417.190879	363665.357833	40.405786
3420.683996	364225.957500	40.410804
3424.163206	364797.084519	40.415821
3427.407235	365347.355395	40.420839
3430.526063	365930.224392	40.425856
3434.436761	366491.389802	40.430874
3437.656068	367081.409715	40.435892
3441.591995	367632.355134	40.440909
3445.189197	368207.987741	40.445927
3448.722239	368780.349400	40.450944
3452.125784	369337.092521	40.455962
3455.759398	369908.332226	40.460980
3458.846747	370466.379520	40.465997
3462.601613	371049.206636	40.471015
3465.944562	371618.439436	40.476032
3470.011131	372161.490961	40.481050
3473.093793	372751.708576	40.486068
3476.570412	373303.795468	40.491085
3480.098536	373875.505612	40.496103
3483.332043	374432.588982	40.501120
3487.055894	374971.514671	40.506125
3489.925933	375494.276835	40.511130
3493.359477	375957.523214	40.516135
3496.111356	376381.343928	40.521140
3498.698125	376729.284852	40.526144
3501.043182	377056.200004	40.531149
3503.480470	377323.552783	40.536154
3505.800598	377542.009583	40.541159
3507.406464	377716.015077	40.546164
3508.969583	377853.246935	40.551168
3510.629250	377960.932601	40.556173
3511.906359	378016.764966	40.561178
3512.657745	378047.117877	40.566183
3514.045695	378054.274879	40.571188
3514.507900	378030.699752	40.576192
3515.386885	377982.564485	40.581197
3516.034941	377920.298152	40.586202
3516.133523	377834.438187	40.591207
3516.552376	377749.112423	40.596212
3516.412545	377636.480686	40.601216
3516.793040	377521.578909	40.606221
3516.991599	377404.111118	40.611226
3517.345653	377245.361507	40.616231
3517.147117	377123.885933	40.621236
3516.798912	376970.511477	40.626240
3516.947073	376819.627012	40.631245
3516.619585	376670.826631	40.636250
3516.722704	376520.049904	40.641255
3516.906258	376357.177611	40.646260
3516.382654	376197.646886	40.651264
3516.186813	376039.284670	40.656269
3516.157991	375885.270541	40.661274
3516.116588	375713.095945	40.666279
3515.004442	375562.685813	40.671284
3514.937821	375406.640887	40.676288
3514.601004	375237.919531	40.681293
3514.027132	375096.529057	40.686298
3513.906261	374953.285870	40.691303
3513.643948	374824.360335	40.696308
3513.136882	374700.993008	40.701312
3513.114431	374562.566004	40.706317
3513.014065	374429.263807	40.711322
3512.878697	374306.726848	40.716327
3512.739256	374167.019683	40.721332
3512.206261	374043.832542	40.726336
3512.235674	373919.564045	40.731341
3511.842347	373809.352896	40.736346
3511.694930	373688.672975	40.741351
3511.517162	373565.402811	40.746356
3511.069349	373465.832497	40.751360
3510.778959	373350.439897	40.756365
3510.390810	373248.163172	40.761370
3510.557826	373151.979957	40.766375
3510.439051	373055.409247	40.771380
3509.852514	372967.942928	40.776384
3509.954634	372862.840391	40.781389
3509.499346	372782.806432	40.786394
3509.426858	372699.379339	40.791399
3509.631835	372609.395904	40.796404
3509.147907	372521.658040	40.801408
3509.272056	372436.800204	40.806413
3509.024352	372361.464242	40.811418
3509.012372	372282.249603	40.816423
3508.630850	372210.317900	40.821428
3508.241135	372147.647164	40.826432
3508.324140	372072.767182	40.831437
3507.977851	371997.293516	40.836442
3507.881775	371924.374951	40.841447
3507.847887	371871.416177	40.846452
3507.627571	371808.209372	40.851456
3507.529424	371742.846262	40.856461
3507.027136	371705.021356	40.861466
3507.044232	371636.638030	40.866471
3507.391295	371600.739341	40.871476
3506.724083	371546.582874	40.876480
3507.046734	371484.587155	40.881485
3507.331115	371443.355968	40.886490
3506.519800	371388.636974	40.891495
3506.924228	371345.936665	40.896500
3506.978641	371291.665791	40.901504
3506.817365	371251.929484	40.906509
3506.404127	371213.555829	40.911514
3506.513536	371153.552183	40.916519
3506.700955	371119.815251	40.921524
3506.286055	371080.805748	40.926528
3506.348864	371020.122410	40.931533
3506.033141	370998.650526	40.936538
3506.196094	370952.146603	40.941543
3506.424749	370922.168073	40.946548
3506.330125	370877.332931	40.951552
3506.081269	370838.449595	40.956557
3505.984008	370810.226975	40.961562
3506.035624	370758.932319	40.966567
3506.171124	370719.326676	40.971572
3506.049859	370700.978442	40.976576
3506.225133	370649.053548	40.981581
3505.978825	370622.711480	40.986586
3505.681762	370581.800337	40.991591
3505.610118	370544.415114	40.996596
3505.430350	370524.498775	41.001600
3505.492470	370483.785155	41.006605
3505.243379	370464.185027	41.011610
3505.251901	370432.765433	41.016615
3505.150164	370419.527436	41.021620
3505.139249	370394.216495	41.026624
3505.518739	370354.597381	41.031629
3505.127858	370347.332609	41.036634
3505.480118	370310.490727	41.041639
3505.062388	370284.608032	41.046644
3504.987486	370261.622179	41.051648
3505.292660	370246.284589	41.056653
3504.763304	370229.934118	41.061658
3505.032115	370199.668891	41.066663
3505.190662	370182.548207	41.071668
3505.130670	370146.432802	41.076672
3504.986223	370134.193637	41.081677
3504.524458	370111.319742	41.086682
3504.825047	370099.773417	41.091687
3505.107482	370075.993206	41.096692
3504.963249	370060.904679	41.101696
3504.912041	370036.083261	41.106701
3505.023293	370030.061946	41.111706
3504.966532	369987.789352	41.116711
3504.908221	369976.884859	41.121716
3504.874408	369957.250466	41.126720
3505.069662	369924.885129	41.131725
3504.914785	369910.154395	41.136730
3504.890246	369890.976432	41.141735
3505.306651	369868.599586	41.146740
3505.018510	369832.469105	41.151744
3505.233978	369810.480161	41.156749
3504.736397	369792.038387	41.161754
3504.816471	369767.017976	41.166759
3505.020235	369759.608215	41.171764
3504.943180	369737.360194	41.176768
3504.920905	369721.692577	41.181773
3504.945382	369705.839480	41.186778
3504.825215	369678.891759	41.191783
3504.831617	369663.931922	41.196788
3504.823361	369639.637735	41.201792
3504.893646	369616.832107	41.206797
3504.608926	369598.229396	41.211802
3504.771167	369578.665598	41.216807
3504.801133	369548.819281	41.221812
3504.727230	369541.351617	41.226816
3504.485903	369518.824166	41.231821
3504.390901	369498.537782	41.236826
3504.585880	369489.297642	41.241831
3504.648737	369466.391347	41.246836
3504.653644	369453.695886	41.251840
3504.581758	369433.711105	41.256845
3504.112818	369426.127788	41.261850
3504.597404	369413.992498	41.266855
3504.478490	369386.408381	41.271860
3504.456687	369382.010771	41.276864
3504.657242	369358.014143	41.281869
3504.574256	369348.538069	41.286874
3504.409781	369322.487554	41.291879
3504.350522	369326.898335	41.296884
3504.052292	369299.749561	41.301888
3504.842874	369293.951477	41.306893
3504.490391	369270.780011	41.311898
3504.443257	369247.356734	41.316903
3504.404190	369247.668374	41.321908
3504.347150	369220.328776	41.326912
3504.184114	369211.653991	41.331917
3504.311247	369206.800325	41.336922
3504.331904	369186.012135	41.341927
3504.430834	369182.256878	41.346932
3504.460821	369176.350055	41.351936
3504.663247	369148.257051	41.356941
3504.075932	369147.815818	41.361946
3503.727024	369123.015497	41.366951
3504.077103	369122.273427	41.371956
3503.853153	369114.422357	41.376960
3504.248800	369110.874594	41.381965
3504.155816	369096.362765	41.386970
3504.710154	369081.366984	41.391975
3504.466453	369063.698868	41.396980
3504.062076	369045.979824	41.401984
3504.283311	369035.437954	41.406989
3504.270265	369031.649504	41.411994
3504.420654	369013.639216	41.416999
3504.474761	369013.452752	41.422004
3504.037447	368988.233835	41.427008
3504.243457	368971.741190	41.432013
3504.074912	368953.119835	41.437018
3504.344806	368956.537305	41.442023
3504.144675	368942.245890	41.447028
3504.379941	368918.014564	41.452032
3504.588979	368914.598049	41.457037
3504.365835	368899.216299	41.462042
3504.399469	368893.461506	41.467047
3504.698120	368876.648888	41.472052
3504.422031	368863.895913	41.477056
3504.501242	368838.289960	41.482061
3504.314203	368833.180629	41.487066
3504.381276	368822.179700	41.492071
3504.280730	368801.461370	41.497076
3504.251382	368790.831850	41.502080
3504.324568	368767.414733	41.507085
3504.241805	368763.281108	41.512090
3504.245276	368742.037485	41.517095
3503.689882	368727.929369	41.522100
3503.953509	368725.699938	41.527104
3503.891956	368707.723030	41.532109
3503.981676	368719.182931	41.537114
3503.877387	368697.829117	41.542119
3504.132721	368686.086041	41.547124
3503.919702	368683.753875	41.552128
3504.376995	368670.070788	41.557133
3504.065724	368670.883404	41.562138
3504.068645	368643.533964	41.567143
3504.141957	368633.804055	41.572148
3503.705986	368625.477594	41.577152
3504.141767	368622.941090	41.582157
3504.377904	368610.005298	41.587162
3504.241007	368600.206849	41.592167
3504.307105	368575.544136	41.597172
3503.990286	368576.561160	41.602176
3504.250225	368560.365127	41.607181
3503.864322	368548.723388	41.612186
3503.713036	368544.956751	41.617191
3504.094288	368526.629912	41.622196
3504.204487	368520.939289	41.627200
3504.345782	368505.983168	41.632205
3503.787553	368501.848361	41.637210
3503.896316	368484.455023	41.642215
3504.052140	368474.610270	41.647220
3504.014023	368456.451465	41.652224
3503.908269	368465.703510	41.657229
3503.908975	368453.695333	41.662234
3503.879718	368444.821156	41.667239
3503.806775	368457.349930	41.672244
3503.863583	368441.084201	41.677248
3503.881695	368416.581631	41.682253
3503.615707	368424.485191	41.687258
3504.017867	368420.529283	41.692263
3504.081055	368404.059002	41.697268
3503.858158	368395.876900	41.702272
3503.801544	368382.402174	41.707277
3503.968018	368380.391615	41.712282
3504.148453	368365.429258	41.717287
3504.254299	368366.964615	41.722292
3503.964559	368350.295696	41.727296
3504.386901	368347.303359	41.732301
3503.992282	368321.110538	41.737306
3503.890742	368305.683913	41.742311
3504.098137	368304.124824	41.747316
3503.638953	368301.322727	41.752320
3503.797037	368289.315066	41.757325
3503.794777	368286.847794	41.762330
3503.876996	368262.360444	41.767335
3503.581160	368261.237088	41.772340
3503.552466	368259.079289	41.777344
3503.992403	368248.350006	41.782349
3503.863008	368246.742393	41.787354
3504.036975	368229.593059	41.792359
3504.035014	368230.458549	41.797364
3503.866234	368215.347818	41.802368
3504.221420	368209.389452	41.807373
3503.766957	368183.663954	41.812378
3503.718337	368182.679603	41.817383
3503.903462	368175.119871	41.822388
3503.888884	368174.282786	41.827392
3504.145737	368158.977540	41.832397
3503.804162	368152.086222	41.837402
3504.042337	368134.799494	41.842407
3504.094744	368113.217091	41.847412
3503.858611	368122.566144	41.852416
3503.800267	368121.176267	41.857421
3503.676012	368096.009107	41.862426
3504.160352	368082.347003	41.867431
3503.786565	368097.136843	41.872436
3504.001695	368075.655903	41.877440
3504.330774	368058.787278	41.882445
3503.754209	368060.990240	41.887450
3503.935780	368036.105436	41.892455
3503.768862	368033.944036	41.897460
3503.670538	368033.832548	41.902464
3503.772518	368017.254224	41.907469
3503.623391	368017.786803	41.912474
3504.083917	368021.912012	41.917479
3503.921922	368021.123671	41.922484
3503.896652	367998.637599	41.927488
3503.998497	367991.727038	41.932493
3503.601509	367991.204820	41.937498
3503.683536	367974.578751	41.942503
3503.985234	367972.699444	41.947508
3504.277022	367961.866305	41.952512
3503.671983	367956.746628	41.957517
3503.822148	367942.857455	41.962522
3504.034486	367935.700444	41.967527
3503.848248	367927.487017	41.972532
3503.555029	367919.875656	41.977536
3504.088263	367910.352733	41.982541
3504.164113	367902.454049	41.987546
3503.962050	367888.569660	41.992551
3503.782430	367882.314175	41.997556
3503.582534	367865.147479	42.002560
3503.810969	367859.463520	42.007565
3503.676150	367862.919616	42.012570
3503.506103	367860.453403	42.017575
3503.862860	367847.065811	42.022580
3503.482268	367836.211731	42.027584
3503.700891	367834.040254	42.032589
3503.523010	367835.874900	42.037594
3503.532267	367834.881391	42.042599
3503.900892	367813.605031	42.047604
3503.720335	367814.447881	42.052608
3503.771558	367805.382761	42.057613
3503.753075	367806.047339	42.062618
3503.945630	367779.659601	42.067623
3503.831456	367784.638934	42.072628
3503.581714	367791.267960	42.077632
3503.862079	367764.306616	42.082637
3503.465459	367757.551146	42.087642
3503.796465	367759.839619	42.092647
3503.942768	367754.957320	42.097652
3503.744593	367745.906174	42.102656
3504.166813	367734.263669	42.107661
3504.112742	367737.121852	42.112666
3503.679435	367717.193421	42.117671
3504.101082	367697.587770	42.122676
3503.631448	367702.419775	42.127680
3504.080339	367677.492507	42.132685
3503.795457	367671.126425	42.137690
3504.168536	367667.073281	42.142695
3504.174348	367647.329814	42.147700
3504.192433	367649.362463	42.152704
3504.170301	367625.908922	42.157709
3503.517440	367609.348010	42.162714
3503.889024	367607.559407	42.167719
3503.817017	367601.007011	42.172724
3503.432779	367586.846026	42.177728
3503.887864	367589.750935	42.182733
3503.657479	367583.452550	42.187738
3503.628584	367584.754819	42.192743
3503.612498	367564.124318	42.197748
3503.763594	367550.718266	42.202752
3503.740257	367543.598449	42.207757
3503.362746	367572.865390	42.212762
3503.716821	367547.138904	42.217767
3503.699623	367531.978531	42.222772
3503.627581	367541.250883	42.227776
3503.938407	367526.801903	42.232781
3503.781346	367525.478497	42.237786
3503.439473	367503.271200	42.242791
3503.603201	367516.144452	42.247796
3503.668823	367508.603499	42.252800
3503.853462	367510.609823	42.257805
3503.635131	367492.987945	42.262810
3503.717846	367478.473245	42.267815
3503.856810	367484.710122	42.272820
3503.580727	367477.630252	42.277824
3503.547634	367457.536666	42.282829
3503.416587	367456.539888	42.287834
3503.308551	367462.943026	42.292839
3503.777305	367463.428814	42.297844
3503.649297	367460.981375	42.302848
3503.855486	367429.706453	42.307853
3503.702413	367439.373263	42.312858
3503.774189	367433.230622	42.317863
3503.807175	367427.195879	42.322868
3504.075711	367416.264515	42.327872
3503.858187	367409.404352	42.332877
3503.971071	367412.261605	42.337882
3503.688950	367385.312628	42.342887
3503.756562	367382.325422	42.347892
3503.453217	367374.919102	42.352896
3503.666685	367367.939913	42.357901
3503.572667	367360.042545	42.362906
3503.852046	367349.084008	42.367911
3503.963472	367353.518888	42.372916
3503.621793	367335.433052	42.377920
3503.777287	367331.134416	42.382925
3503.488436	367310.597801	42.387930
3503.675469	367316.547243	42.392935
3503.745824	367317.604853	42.397940
3503.436392	367302.388835	42.402944
3504.028953	367283.086724	42.407949
3503.475686	367304.876275	42.412954
3503.836139	367291.564256	42.417959
3503.871986	367276.777038	42.422964
3503.352168	367276.274229	42.427968
3503.656408	367266.125882	42.432973
3503.502590	367271.874797	42.437978
3503.554932	367256.067289	42.442983
3503.445780	367247.129176	42.447988
3503.365865	367239.941929	42.452992
3503.888405	367233.371812	42.457997
3503.710115	367252.227174	42.463002
3503.747766	367236.600075	42.468007
3503.654546	367219.925101	42.473012
3503.747920	367214.491388	42.478016
3503.790589	367216.494728	42.483021
3503.746080	367213.067282	42.488026
3503.735250	367193.936849	42.493031
3503.571957	367193.225024	42.498036
3503.819633	367201.912622	42.503040
3503.976250	367183.926041	42.508045
3503.583696	367167.858091	42.513050
3503.355911	367164.561383	42.518055
3503.673591	367166.851994	42.523060
3503.733559	367169.768511	42.528064
3503.885076	367143.107020	42.533069
3503.823576	367140.191093	42.538074
3503.839906	367134.158944	42.543079
3503.786633	367109.946793	42.548084
3503.685583	367102.610214	42.553088
3503.895324	367098.124885	42.558093
3503.467149	367102.594213	42.563098
3503.524431	367084.979483	42.568103
3504.021574	367077.777308	42.573108
3503.734880	367077.313968	42.578112
3503.460452	367081.606339	42.583117
3503.375301	367063.428953	42.588122
3503.852867	367054.347162	42.593127
3503.512194	367056.818184	42.598132
3503.364858	367059.055106	42.603136
3503.754302	367046.603458	42.608141
3503.670747	367044.301620	42.613146
3503.672089	367025.652588	42.618151
3503.791756	367021.385028	42.623156
3503.466424	367014.490964	42.628160
3503.596595	367026.479193	42.633165
3503.457235	367001.491891	42.638170
3503.480571	367005.660869	42.643175
3503.593409	366995.339183	42.648180
3503.570386	367000.991129	42.653184
3503.981929	366992.275952	42.658189
3503.562216	366978.247589	42.663194
3503.643031	366976.072414	42.668199
3503.527644	366968.381891	42.673204
3503.461086	366967.451232	42.678208
3503.843749	366970.952799	42.683213
3503.567413	366955.426124	42.688218
3503.729856	366934.919757	42.693223
3503.932633	366946.031500	42.698228
3503.634839	366934.629824	42.703232
3503.709506	366914.646166	42.708237
3503.395006	366909.633086	42.713242
3503.511550	366906.943418	42.718247
3503.660561	366909.311592	42.723252
3503.373032	366900.019977	42.728256
3503.557623	366886.328566	42.733261
3503.801542	366890.615336	42.738266
3503.279195	366874.389704	42.743271
3503.502650	366880.664194	42.748276
3503.383726	366877.070391	42.753280
3503.832953	366878.755053	42.758285
3503.732711	366863.887443	42.763290
3503.565067	366854.627750	42.768295
3503.453653	366863.626605	42.773300
3503.337183	366861.991456	42.778304
3503.983490	366842.629773	42.783309
3503.586434	366846.000195	42.788314
3503.582396	366833.610694	42.793319
3503.887613	366827.660044	42.798324
3503.622331	366816.202313	42.803329
3503.702538	366797.286296	42.808333
3503.661076	366803.119277	42.813338
3503.816592	366803.832689	42.818343
3503.612205	366779.593364	42.823348
3503.101387	366784.381094	42.828353
3503.706526	366776.296764	42.833357
3503.547163	366787.923757	42.838362
3503.361083	366772.535402	42.843367
3503.767358	366773.692572	42.848372
3503.703851	366763.093405	42.853377
3503.789192	366743.336962	42.858381
3503.784178	366741.887725	42.863386
3503.835591	366743.889705	42.868391
3503.531617	366729.868408	42.873396
3503.705387	366721.216210	42.878401
3503.782297	366717.387897	42.883405
3503.939049	366714.335670	42.888410
3503.537633	366711.066378	42.893415
3503.755084	366694.265765	42.898420
3503.531926	366697.837686	42.903425
3503.432400	366695.131279	42.908429
3503.622146	366695.076015	42.913434
3503.931215	366663.733404	42.918439
3503.702478	366670.079412	42.923444
3503.554597	366659.264578	42.928449
3503.552648	366645.602583	42.933453
3503.583508	366638.372285	42.938458
3503.624702	366623.685773	42.943463
3503.772963	366629.081708	42.948468
3503.384094	366633.926501	42.953473
3503.447426	366621.653502	42.958477
3503.582578	366609.063838	42.963482
3503.710896	366597.365731	42.968487
3503.719221	366611.663139	42.973492
3503.545992	366612.759275	42.978497
3503.561042	366591.003939	42.983501
3503.566570	366583.675867	42.988506
3503.717157	366574.823766	42.993511
3503.390376	366561.925483	42.998516
3503.056767	366582.713854	43.003521
3503.164303	366570.332084	43.008525
3503.330169	366578.701988	43.013530
3503.470799	366575.474204	43.018535
3503.707613	366550.783370	43.023540
3503.354916	366556.334837	43.028545
3503.627440	366540.619478	43.033549
3503.933514	366551.664105	43.038554
3503.843770	366544.859934	43.043559
3503.675818	366515.882438	43.048564
3503.526550	366521.045557	43.053569
3503.311127	366517.314327	43.058573
3503.553572	366538.342400	43.063578
3503.633173	366508.358956	43.068583
3503.651347	366497.008985	43.073588
3503.353924	366488.202252	43.078593
3503.630015	366487.268298	43.083597
3503.458382	366482.792315	43.088602
3503.161439	366480.829491	43.093607
3503.645294	366463.477828	43.098612
3503.398046	366465.069073	43.103617
3503.090773	366466.771578	43.108621
3503.337975	366449.050245	43.113626
3503.088110	366463.439403	43.118631
3503.540378	366459.882478	43.123636
3503.360896	366468.561423	43.128641
3503.570031	366461.837200	43.133645
3503.281072	366461.654076	43.138650
3503.454099	366436.464416	43.143655
3503.519219	366435.360275	43.148660
3503.338395	366439.765122	43.153665
3503.832171	366435.769113	43.158669
3503.450957	366447.940114	43.163674
3503.106987	366438.377459	43.168679
3503.351283	366431.367808	43.173684
3503.102569	366426.980332	43.178689
3503.696145	366404.242963	43.183693
3503.339569	366415.672248	43.188698
3502.951767	366414.487056	43.193703
3503.576099	366420.214831	43.198708
3503.569309	366420.826696	43.203713
3503.765089	366422.983963	43.208717
3503.859644	366405.668381	43.213722
3503.432282	366398.815793	43.218727
3503.700742	366389.258077	43.223732
3503.562969	366397.192613	43.228737
3503.786333	366383.418590	43.233741
3503.399791	366370.860450	43.238746
3503.233712	366371.217632	43.243751
3503.623247	366372.504672	43.248756
3503.470025	366369.781292	43.253761
3503.906212	366367.880657	43.258765
3503.370230	366354.023133	43.263770
3503.738905	366338.343387	43.268775
3504.015977	366337.816353	43.273780
3503.605538	366336.863719	43.278785
3503.968514	366306.479147	43.283789
3503.869041	366309.370042	43.288794
3503.757532	366305.266172	43.293799
3503.668286	366298.970734	43.298804
3503.673994	366280.015390	43.303809
3503.631892	366281.141689	43.308813
3503.318929	366287.679163	43.313818
3503.421818	366293.692930	43.318823
3503.776066	366263.284266	43.323828
3503.276992	366264.788118	43.328833
3503.952185	366247.075371	43.333837
3503.548803	366256.247717	43.338842
3503.662308	366248.698980	43.343847
3503.613356	366229.294293	43.348852
3503.509554	366219.820835	43.353857
3503.536326	366204.907483	43.358861
3503.465903	366225.603528	43.363866
3503.845806	366218.775945	43.368871
3503.643128	366195.731828	43.373876
3503.262012	366196.402875	43.378881
3503.728583	366181.267332	43.383885
3503.497866	366187.461066	43.388890
3503.305870	366187.975001	43.393895
3503.657010	366186.876522	43.398900
3503.068710	366170.915484	43.403905
3503.662609	366155.887016	43.408909
3503.100514	366160.148625	43.413914
3503.279544	366161.189083	43.418919
3503.571906	366148.218241	43.423924
3503.365718	366161.404793	43.428929
3503.539886	366155.932735	43.433933
3503.561409	366162.849871	43.438938
3503.533567	366132.908604	43.443943
3503.666180	366139.935394	43.448948
3503.255093	366141.857862	43.453953
3503.060802	366120.618800	43.458957
3502.890130	366135.504394	43.463962
3503.128437	366136.306498	43.468967
3503.234699	366125.222374	43.473972
3503.250479	366137.686894	43.478977
3503.288268	366139.512956	43.483981
3503.540648	366146.749793	43.488986
3503.344437	366132.202422	43.493991
3503.307244	366112.643169	43.498996
3503.114823	366108.755613	43.504001
3503.356219	366092.892363	43.509005
3503.230299	366104.946769	43.514010
3503.580856	366116.086242	43.519015
3503.613340	366116.488362	43.524020
3503.783500	366106.997012	43.529025
3503.745054	366091.228886	43.534029
3503.511083	366083.429744	43.539034
3503.559553	366090.520729	43.544039
3503.632002	366077.050339	43.549044
3503.329969	366089.107149	43.554049
3503.320640	366054.456030	43.559053
3503.637025	366055.551103	43.564058
3503.289212	366057.489015	43.569063
3503.318292	366052.955815	43.574068
3503.053639	366070.197005	43.579073
3503.332161	366066.209551	43.584077
3503.430114	366067.084730	43.589082
3503.346483	366060.483060	43.594087
3503.512834	366059.286578	43.599092
3503.008879	366036.646205	43.604097
3503.442154	366027.800191	43.609101
3503.432875	366032.814023	43.614106
3503.397875	366038.951393	43.619111
3503.651479	366029.192409	43.624116
3503.662212	366041.734080	43.629121
3503.553532	366028.928375	43.634125
3503.424268	366030.908065	43.639130
3503.143779	366007.799825	43.644135
3503.356175	366020.106081	43.649140
3503.291541	366020.676211	43.654145
3503.560488	366010.380503	43.659149
3503.471216	366021.157008	43.664154
3503.479497	366012.810703	43.669159
3503.340872	365996.803956	43.674164
3503.618311	365983.733655	43.679169
3503.612815	365976.076473	43.684173
3503.381033	365988.300302	43.689178
3503.518758	365986.319623	43.694183
3503.608513	365975.645154	43.699188
3503.457613	365971.929120	43.704193
3503.884752	365955.349506	43.709197
3503.551261	365954.511912	43.714202
3503.392499	365972.168923	43.719207
3503.312596	365959.918387	43.724212
3503.347348	365950.575624	43.729217
3503.624371	365937.505375	43.734221
3503.135353	365933.868235	43.739226
3503.457205	365927.940278	43.744231
3503.710875	365927.544153	43.749236
3503.574807	365937.310370	43.754241
3503.535210	365918.870889	43.759245
3503.513267	365912.793740	43.764250
3503.634260	365891.377512	43.769255
3503.575923	365885.560539	43.774260
3503.690746	365889.893258	43.779265
3503.370124	365880.911974	43.784269
3503.412774	365870.957321	43.789274
3503.527675	365873.280058	43.794279
3503.418235	365865.410305	43.799284
3503.181458	365868.170279	43.804289
3503.442715	365860.063822	43.809293
3503.346643	365871.681047	43.814298
3502.995019	365876.240164	43.819303
3503.570544	365873.910398	43.824308
3503.233541	365869.562268	43.829313
3503.190879	365848.197334	43.834317
3503.307266	365855.837358	43.839322
3503.166107	365852.501415	43.844327
3503.492814	365854.358142	43.849332
3503.338030	365857.156040	43.854337
3503.535538	365859.847358	43.859341
3503.377941	365862.493044	43.864346
3503.606479	365849.710304	43.869351
3503.525131	365842.802928	43.874356
3503.508539	365826.725943	43.879361
3503.585086	365822.185215	43.884365
3503.106991	365825.339541	43.889370
3503.218623	365831.351987	43.894375
3503.198808	365825.834229	43.899380
3503.267865	365835.797025	43.904385
3503.705724	365823.159285	43.909389
3503.665118	365818.866062	43.914394
3503.208069	365804.639691	43.919399
3503.409651	365802.419924	43.924404
3503.348726	365791.692904	43.929409
3503.761741	365796.512787	43.934413
3503.591759	365804.045436	43.939418
3503.410697	365787.994438	43.944423
3503.603540	365772.520391	43.949428
3503.286073	365777.684744	43.954433
3503.333517	365774.344421	43.959437
3503.434442	365770.715773	43.964442
3503.467705	365774.985068	43.969447
3503.449814	365770.968120	43.974452
3503.198939	365750.933637	43.979457
3503.609520	365746.823506	43.984461
3503.264211	365741.815165	43.989466
3503.345083	365738.291456	43.994471
3503.660584	365742.617906	43.999476
3503.274923	365752.067423	44.004481
3503.523900	365741.749368	44.009485
3503.412705	365728.969418	44.014490
3503.298337	365714.688843	44.019495
3503.286776	365713.698578	44.024500
3503.260628	365712.099993	44.029505
3503.373716	365707.706134	44.034509
3503.232289	365719.915751	44.039514
3502.934423	365719.352390	44.044519
3503.226863	365716.354973	44.049524
3503.168261	365713.463937	44.054529
3503.369310	365720.250989	44.059533
3503.681498	365721.397619	44.064538
3503.508275	365709.238096	44.069543
3503.536457	365692.187158	44.074548
3503.394676	365692.947589	44.079553
3503.440973	365686.299880	44.084557
3503.401677	365692.005449	44.089562
3503.337702	365694.102046	44.094567
3503.391613	365696.103678	44.099572
3503.129052	365671.694849	44.104577
3503.652800	365656.346548	44.109581
3503.365745	365661.480663	44.114586
3503.601007	365658.695824	44.119591
3503.060525	365664.277088	44.124596
3503.192740	365676.952313	44.129601
3503.902243	365664.653226	44.134605
3503.375610	365659.342785	44.139610
3503.493298	365657.441588	44.144615
3503.853180	365626.064775	44.149620
3503.603268	365643.049370	44.154625
3503.455548	365636.406884	44.159629
3503.516798	365642.427321	44.164634
3503.708927	365623.620328	44.169639
3503.700388	365606.066307	44.174644
3503.373746	365595.483020	44.179649
3503.510693	365601.618709	44.184653
3503.529383	365602.735414	44.189658
3503.425844	365587.817016	44.194663
3503.713041	365578.256166	44.199668
3503.559234	365566.958591	44.204673
3503.739738	365563.241017	44.209677
3503.402391	365576.448475	44.214682
3503.541834	365555.461699	44.219687
3503.368782	365533.582930	44.224692
3503.134028	365532.017317	44.229697
3503.371364	365530.504285	44.234701
3503.469827	365535.653796	44.239706
3503.046897	365529.029359	44.244711
3503.170686	365544.377454	44.249716
3503.180795	365537.048487	44.254721
3503.398766	365534.597130	44.259725
3503.281095	365551.815282	44.264730
3503.483166	365536.237924	44.269735
3503.337521	365512.573811	44.274740
3503.193447	365515.548137	44.279745
3503.151302	365515.478646	44.284749
3503.362973	365516.895602	44.289754
3503.345337	365515.015792	44.294759
3503.314530	365521.737757	44.299764
3503.272506	365520.854075	44.304769
3503.348623	365518.857672	44.309773
3503.377530	365524.679695	44.314778
3503.427739	365515.258070	44.319783
3503.903463	365495.083160	44.324788
3503.169789	365489.958088	44.329793
3503.548077	365488.728086	44.334797
3503.614403	365483.272996	44.339802
3503.566703	365487.834990	44.344807
3503.383368	365467.026416	44.349812
3503.291888	365452.131509	44.354817
3503.583441	365449.846616	44.359821
3503.736243	365465.393694	44.364826
3503.411834	365454.581034	44.369831
3503.493322	365463.371573	44.374836
3503.502788	365445.661986	44.379841
3503.131001	365427.783679	44.384845
3503.223329	365427.718371	44.389850
3503.466607	365420.988596	44.394855
3503.459702	365424.297444	44.399860
3503.728870	365428.173276	44.404865
3503.795640	365420.784447	44.409869
3503.356293	365416.325237	44.414874
3503.376074	365397.494512	44.419879
3503.638393	365395.977526	44.424884
3503.453960	365399.543427	44.429889
3503.609527	365402.699376	44.434893
3503.149113	365419.437461	44.439898
3503.081987	365388.458749	44.444903
3503.166226	365369.108962	44.449908
3503.149675	365370.002257	44.454913
3503.081848	365354.594719	44.459917
3503.217217	365378.260890	44.464922
3503.086760	365376.373468	44.469927
3503.524750	365372.996816	44.474932
3503.135174	365370.717828	44.479937
3503.630598	365372.420688	44.484941
3503.486915	365379.847478	44.489946
3503.542715	365368.262286	44.494951
3503.736986	365368.918709	44.499956
3503.552003	365344.929969	44.504961
3503.692462	365336.282770	44.509965
3503.867471	365344.676902	44.514970
3503.659382	365321.633192	44.519975
3503.454834	365315.304958	44.524980
3503.123559	365305.434738	44.529985
3503.755487	365307.217792	44.534989
3503.370613	365300.968950	44.539994
3503.490470	365313.442687	44.544999
3503.397050	365315.365855	44.550004
3503.425385	365288.620961	44.555009
3503.696483	365277.586899	44.560013
3503.684012	365278.606766	44.565018
3503.236836	365283.486364	44.570023
3503.771456	365271.850894	44.575028
3503.467525	365274.799622	44.580033
3503.275095	365251.371755	44.585037
3503.253798	365239.900492	44.590042
3503.437768	365247.962466	44.595047
3503.364083	365243.954291	44.600052
3502.951273	365266.155159	44.605057
3503.537758	365251.000347	44.610061
3503.472181	365256.786456	44.615066
3503.314779	365257.244046	44.620071
3503.430825	365232.597023	44.625076
3503.371593	365229.400740	44.630081
3503.286779	365229.007235	44.635085
3503.491321	365227.346719	44.640090
3503.319002	365223.913883	44.645095
3503.584743	365232.980654	44.650100
3503.528539	365233.396804	44.655105
3503.685698	365216.477955	44.660109
3503.543928	365212.175225	44.665114
3502.953856	365195.120068	44.670119
3503.312409	365187.201654	44.675124
3503.357756	365192.715804	44.680129
3503.570228	365199.857331	44.685133
3503.356145	365204.191227	44.690138
3503.469645	365182.139770	44.695143
3503.346675	365169.539625	44.700148
3503.635021	365165.804969	44.705153
3503.691250	365157.985231	44.710157
3503.309953	365164.609999	44.715162
3503.033149	365165.569886	44.720167
3503.523103	365159.157277	44.725172
3503.635736	365161.760283	44.730177
3503.719668	365134.675749	44.735181
3503.139602	365136.523201	44.740186
3503.303402	365120.264786	44.745191
3503.502878	365119.342918	44.750196
3503.499965	365126.696608	44.755201
3503.666809	365123.490020	44.760205
3503.623316	365110.953622	44.765210
3503.171752	365099.143255	44.770215
3503.471952	365090.063666	44.775220
3503.188273	365096.393137	44.780225
3503.384086	365092.189685	44.785229
3503.382033	365097.609568	44.790234
3503.295758	365099.429844	44.795239
3503.780076	365103.449793	44.800244
3503.743333	365090.149029	44.805249
3503.848648	365063.468162	44.810253
3503.527657	365076.495078	44.815258
3503.321318	365056.478688	44.820263
3503.455998	365047.756018	44.825268
3503.401318	365031.354010	44.830273
3503.476521	365032.003818	44.835277
3503.285433	365031.143692	44.840282
3503.260775	365034.226386	44.845287
3503.471692	365030.478518	44.850292
3503.088198	365046.110525	44.855297
3503.300734	365032.337802	44.860301
3503.452532	365042.465794	44.865306
3503.341141	365019.890063	44.870311
3503.510636	365006.989204	44.875316
3503.081408	365004.233045	44.880321
3503.510550	365001.646503	44.885325
3503.273657	365004.584650	44.890330
3503.067105	365011.385361	44.895335
3503.619491	365006.260462	44.900340
3503.521775	365014.061692	44.905345
3503.355650	364995.565507	44.910349
3503.140757	364986.618216	44.915354
3503.074615	364980.013622	44.920359
3503.044796	364982.715488	44.925364
3503.229020	364977.776006	44.930369
3503.083057	364972.888723	44.935373
3503.139077	364988.095061	44.940378
3502.796927	364981.457773	44.945383
3503.147655	364975.932217	44.950388
3503.101548	364990.696723	44.955393
3503.026361	364978.241629	44.960397
3503.013324	364982.009456	44.965402
3502.883904	364985.490363	44.970407
3503.444877	364990.694033	44.975412
3503.449506	364983.467615	44.980417
3503.420539	364991.817730	44.985421
3503.214630	364990.705515	44.990426
3503.193898	364991.624922	44.995431
3503.555450	364998.717469	45.000436
3503.187476	364999.666329	45.005441
3503.395790	364993.552654	45.010445
3503.233184	364977.294904	45.015450
3503.155310	364962.601231	45.020455
3503.279648	364965.762147	45.025460
3502.539592	364968.423638	45.030465
3503.381171	364961.014015	45.035469
3503.014259	364978.017356	45.040474
3503.306663	364959.932087	45.045479
3503.560316	364968.390186	45.050484
3503.228017	364963.227042	45.055489
3503.295317	364971.434726	45.060493
3503.271356	364965.892076	45.065498
3503.282990	364968.867264	45.070503
3503.488358	364971.633722	45.075508
3503.317307	364970.694098	45.080513
3503.423949	364960.296594	45.085517
3503.532261	364958.091532	45.090522
3503.337200	364946.851210	45.095527
3503.756659	364951.364847	45.100532
3503.461402	364939.911375	45.105537
3503.580546	364942.742353	45.110541
3503.448482	364930.041805	45.115546
3503.192945	364922.118655	45.120551
3503.229863	364912.648119	45.125556
3503.207216	364919.623314	45.130561
3503.382525	364900.437033	45.135565
3503.502629	364919.475190	45.140570
3503.328236	364926.754250	45.145575
3503.602050	364912.233949	45.150580
3503.352185	364920.949762	45.155585
3503.275419	364892.592885	45.160589
3503.274902	364891.270094	45.165594
3503.363635	364881.511484	45.170599
3503.338281	364893.219553	45.175604
3503.126698	364891.243163	45.180609
3503.298740	364884.575456	45.185613
3503.195158	364886.754681	45.190618
3503.567793	364886.517843	45.195623
3503.488133	364890.932291	45.200628
3503.419382	364876.924114	45.205633
3503.514598	364860.498347	45.210637
3503.147493	364845.621371	45.215642
3503.209302	364858.994924	45.220647
3503.341060	364854.699804	45.225652
3503.073320	364867.158610	45.230657
3503.429363	364849.165009	45.235661
3503.744686	364858.173131	45.240666
3503.549226	364862.046136	45.245671
3503.607493	364837.891455	45.250676
3503.144159	364837.608674	45.255681
3503.335388	364830.887041	45.260685
3503.148854	364828.804914	45.265690
3503.236226	364827.417341	45.270695
3503.293317	364826.492533	45.275700
3502.868437	364832.920694	45.280705
3503.164606	364823.638142	45.285709
3503.575831	364847.566299	45.290714
3503.294909	364840.257785	45.295719
3503.483948	364834.961320	45.300724
3503.401407	364821.031637	45.305729
3503.418083	364800.598228	45.310733
3503.309580	364813.388080	45.315738
3503.299676	364804.840881	45.320743
3503.397590	364809.558026	45.325748
3502.978748	364814.407752	45.330753
3503.159246	364802.497383	45.335757
3503.553014	364802.409863	45.340762
3503.632236	364805.170831	45.345767
3503.393777	364780.834040	45.350772
3503.305841	364778.863541	45.355777
3503.312844	364769.932013	45.360781
3503.277848	364784.262294	45.365786
3503.438965	364771.439022	45.370791
3503.368306	364783.663148	45.375796
3503.077646	364775.338432	45.380801
3503.350076	364779.315578	45.385805
3503.517921	364772.699405	45.390810
3503.408421	364769.969016	45.395815
3503.669672	364747.359681	45.400820
3503.470629	364751.614912	45.405825
3503.436351	364735.209571	45.410829
3503.101809	364753.632704	45.415834
3503.082288	364743.255096	45.420839
3503.420503	364741.547987	45.425844
3503.106019	364752.920152	45.430849
3503.292839	364745.308687	45.435853
3503.068044	364719.824754	45.440858
3503.110081	364721.522986	45.445863
3503.491883	364710.547615	45.450868
3503.493496	364721.768041	45.455873
3503.666616	364715.990656	45.460877
3503.449071	364719.892609	45.465882
3503.256858	364723.892330	45.470887
3503.745714	364717.250843	45.475892
3503.332996	364698.310098	45.480897
3503.831443	364682.812809	45.485901
3503.618717	364685.721712	45.490906
3503.478440	364676.635347	45.495911
3503.492153	364677.091334	45.500916
3503.369805	364660.394570	45.505921
3503.655301	364647.729704	45.510925
3503.269312	364647.587353	45.515930
3502.886300	364648.614928	45.520935
3503.273263	364653.159175	45.525940
3503.062145	364660.571301	45.530945
3503.045501	364657.190141	45.535949
3502.946183	364647.232220	45.540954
3503.402994	364652.554169	45.545959
3503.452392	364648.144833	45.550964
3503.273691	364657.536417	45.555969
3503.275209	364652.498566	45.560973
3503.356805	364656.709440	45.565978
3503.165526	364639.107604	45.570983
3503.465227	364620.690283	45.575988
3503.204096	364630.705544	45.580993
3503.502099	364621.168228	45.585997
3503.111601	364623.443712	45.591002
3503.164420	364623.944404	45.596007
3503.379663	364626.887426	45.601012
3503.119306	364629.422212	45.606017
3503.888286	364615.943045	45.611021
3503.305116	364634.481862	45.616026
3503.430837	364604.006436	45.621031
3503.510443	364597.353302	45.626036
3503.205221	364602.261418	45.631041
3503.355172	364590.584813	45.636045
3503.596211	364591.030306	45.641050
3503.388851	364593.378612	45.646055
3503.713398	364587.780819	45.651060
3503.276580	364575.077465	45.656065
3503.329050	364557.182628	45.661069
3503.301762	364566.143198	45.666074
3503.564598	364561.318460	45.671079
3503.576652	364560.502540	45.676084
3503.388890	364572.897896	45.681089
3503.361448	364579.568581	45.686093
3503.504517	364565.704925	45.691098
3503.588683	364556.557610	45.696103
3503.416413	364559.358351	45.701108
3503.082928	364567.349592	45.706113
3503.439491	364563.705877	45.711117
3503.528673	364563.361189	45.716122
3503.137703	364572.659130	45.721127
3503.632223	364559.325109	45.726132
3503.379106	364541.427691	45.731137
3503.525372	364524.612080	45.736141
3503.627961	364527.293040	45.741146
3503.193301	364522.044255	45.746151
3503.559604	364528.245604	45.751156
3503.312163	364520.041226	45.756161
3503.685671	364515.326204	45.761165
3503.462342	364510.959970	45.766170
3503.357736	364502.707564	45.771175
3503.817493	364502.304291	45.776180
3503.452970	364511.903385	45.781185
3503.487227	364492.586570	45.786189
3503.459050	364481.446967	45.791194
3503.355530	364460.192773	45.796199
3503.794752	364456.841303	45.801204
3503.174586	364470.246455	45.806209
3503.510498	364466.351562	45.811213
3503.558191	364456.955557	45.816218
3503.058944	364448.638314	45.821223
3503.411300	364428.660539	45.826228
3503.374909	364433.119077	45.831233
3503.261306	364413.265847	45.836237
3503.192210	364416.813592	45.841242
3503.280923	364410.871408	45.846247
3503.350512	364423.811319	45.851252
3503.326327	364431.855459	45.856257
3503.421548	364438.761208	45.861261
3503.245264	364447.643582	45.866266
3503.379184	364425.563088	45.871271
3503.358690	364395.212412	45.876276
3503.121296	364389.448998	45.881281
3503.047022	364395.796348	45.886285
3503.223446	364403.935996	45.891290
3503.721863	364396.682308	45.896295
3503.783237	364404.407605	45.901300
3503.338835	364405.088680	45.906305
3503.661165	364396.539768	45.911309
3503.498087	364378.475390	45.916314
3503.535692	364374.271440	45.921319
3503.343112	364369.366018	45.926324
3503.460319	364366.930530	45.931329
3503.471076	364375.020043	45.936333
3503.432369	364376.680166	45.941338
3503.056910	364354.909157	45.946343
3503.261031	364335.590865	45.951348
3503.441637	364340.549421	45.956353
3503.372151	364327.024619	45.961357
3503.180888	364337.156116	45.966362
3503.121663	364332.687592	45.971367
3503.806018	364331.358286	45.976372
3503.477410	364342.681898	45.981377
3503.539254	364316.261901	45.986381
3503.022178	364315.402410	45.991386
3503.226337	364298.552120	45.996391
3503.375422	364298.910380	46.001396
3503.031626	364301.076722	46.006401
3503.159238	364302.430674	46.011405
3503.224108	364304.227086	46.016410
3502.859727	364300.366560	46.021415
3502.882202	364309.624636	46.026420
3503.234231	364321.680287	46.031425
3503.510631	364303.241078	46.036429
3503.014779	364316.906501	46.041434
3503.340515	364315.811994	46.046439
3503.701765	364298.758765	46.051444
3503.527354	364312.373371	46.056449
3503.657447	364286.629542	46.061453
3503.392228	364285.806565	46.066458
3503.025186	364272.099796	46.071463
3503.331682	364271.771637	46.076468
3503.469971	364279.026811	46.081473
3503.465810	364280.070831	46.086477
3503.216063	364285.453638	46.091482
3503.366441	364275.023620	46.096487
3503.305583	364258.520536	46.101492
3503.237066	364253.620931	46.106497
3503.576461	364243.186468	46.111501
3503.172212	364253.682422	46.116506
3503.254211	364250.972614	46.121511
3503.230636	364247.999616	46.126516
3503.210766	364252.659109	46.131521
3503.658002	364233.378670	46.136525
3503.653808	364246.457514	46.141530
3503.184934	364233.123042	46.146535
3503.470627	364220.788793	46.151540
3503.324653	364224.119714	46.156545
3503.609034	364211.251354	46.161549
3503.355780	364224.471353	46.166554
3502.845284	364223.738039	46.171559
3503.173122	364225.136671	46.176564
3502.960635	364227.053264	46.181569
3503.280608	364217.028963	46.186573
3503.378513	364220.499434	46.191578
3503.303068	364218.526935	46.196583
3503.654592	364210.533132	46.201588
3503.359609	364194.881233	46.206593
3503.102910	364192.504847	46.211597
3503.276621	364182.045676	46.216602
3503.207459	364182.540214	46.221607
3503.376197	364192.233176	46.226612
3502.931152	364191.998385	46.231617
3503.518733	364182.745965	46.236621
3503.421407	364189.325981	46.241626
3502.959039	364189.475584	46.246631
3502.863520	364194.579583	46.251636
3502.772383	364199.352123	46.256641
3503.027274	364200.253415	46.261645
3502.994998	364201.632648	46.266650
3503.010703	364200.332716	46.271655
3503.306472	364206.163607	46.276660
3503.254547	364219.021012	46.281665
3503.193035	364212.339243	46.286669
3503.239932	364223.705295	46.291674
3503.117138	364206.423232	46.296679
3503.440751	364197.823193	46.301684
3503.488926	364179.496346	46.306689
3503.100490	364152.155138	46.311693
3503.372679	364151.450748	46.316698
3503.235075	364140.837234	46.321703
3503.297775	364149.707328	46.326708
3503.042074	364162.851401	46.331713
3503.323318	364147.795367	46.336717
3503.111717	364152.154414	46.341722
3503.133475	364158.715608	46.346727
3503.189558	364159.317564	46.351732
3503.144538	364161.080467	46.356737
3503.340250	364147.564573	46.361741
3503.343684	364169.903718	46.366746
3503.396748	364156.155942	46.371751
3503.699424	364135.753352	46.376756
3503.081002	364135.164317	46.381761
3503.228899	364130.383148	46.386765
3503.516807	364124.154999	46.391770
3503.309979	364126.961230	46.396775
3503.534009	364124.788721	46.401780
3502.932475	364136.460856	46.406785
3503.271241	364131.395076	46.411789
3503.384218	364137.890964	46.416794
3503.187642	364117.592737	46.421799
3503.494860	364101.031406	46.426804
3503.198692	364107.362989	46.431809
3503.440849	364097.910724	46.436813
3503.638400	364095.487963	46.441818
3503.211459	364098.100001	46.446823
3503.490475	364094.621170	46.451828
3503.653471	364088.412765	46.456833
3503.433632	364079.389745	46.461837
3503.436634	364065.166427	46.466842
3503.583764	364069.748649	46.471847
3503.620601	364062.924092	46.476852
3503.256318	364068.375919	46.481857
3503.463150	364049.998495	46.486861
3503.259038	364037.334532	46.491866
3503.150413	364026.970848	46.496871
3503.104098	364025.019179	46.501876
3503.305433	364037.047842	46.506881
3503.290456	364024.201313	46.511885
3503.424243	364041.431170	46.516890
3503.393173	364035.304325	46.521895
3503.582261	364036.241467	46.526900
3503.201502	364039.533188	46.531905
3503.260309	364035.376742	46.536909
3503.616797	364014.812929	46.541914
3503.396240	364009.403017	46.546919
3503.468031	364009.544505	46.551924
3503.147437	364002.420234	46.556929
3503.521305	363998.417526	46.561933
3503.245924	364010.470674	46.566938
3503.223200	363998.007018	46.571943
3503.378936	364006.582551	46.576948
3503.259695	363991.488004	46.581953
3503.398998	363977.650210	46.586957
3503.449574	363977.133515	46.591962
3503.174119	363975.421619	46.596967
3503.402831	363969.940677	46.601972
3503.422923	363973.347137	46.606977
3503.603721	363970.443586	46.611981
3503.110594	363976.195675	46.616986
3503.052737	363980.377769	46.621991
3503.399838	363967.728420	46.626996
3502.967999	363943.701636	46.632001
3503.181271	363935.118991	46.637005
3503.533745	363938.930895	46.642010
3503.153989	363932.502948	46.647015
3503.362098	363933.004541	46.652020
3503.163551	363932.094686	46.657025
3503.317360	363939.805448	46.662029
3503.023001	363947.179961	46.667034
3502.793376	363940.372068	46.672039
3503.097198	363938.415929	46.677044
3502.937504	363941.087501	46.682049
3502.924849	363939.232283	46.687053
3503.044074	363948.246143	46.692058
3502.977871	363946.781046	46.697063
3503.005102	363948.201766	46.702068
3503.051971	363946.362582	46.707073
3503.299067	363941.413048	46.712077
3502.924779	363946.255821	46.717082
3502.940040	363946.889678	46.722087
3503.527894	363945.422955	46.727092
3503.203206	363955.855511	46.732097
3503.478803	363953.140523	46.737101
3503.196336	363954.482985	46.742106
3503.335586	363956.496646	46.747111
3503.347258	363955.629888	46.752116
3503.064178	363950.331629	46.757121
3502.770223	363941.956394	46.762125
3503.222316	363950.637748	46.767130
3503.250862	363943.127502	46.772135
3503.599302	363920.249537	46.777140
3502.956832	363922.666665	46.782145
3503.110912	363914.195150	46.787149
3503.197879	363919.728318	46.792154
3503.190712	363925.327255	46.797159
3503.260620	363919.489755	46.802164
3503.115274	363926.917045	46.807169
3503.453983	363916.889716	46.812173
3503.184263	363929.196427	46.817178
3503.019718	363929.756935	46.822183
3503.541511	363920.514863	46.827188
3503.258185	363932.620174	46.832193
3503.268455	363923.153645	46.837197
3503.171326	363921.235450	46.842202
3503.242842	363919.901243	46.847207
3503.068087	363911.329051	46.852212
3502.908081	363901.227899	46.857217
3503.252215	363894.965386	46.862221
3503.045562	363896.244977	46.867226
3503.114931	363900.686847	46.872231
3503.094631	363904.735792	46.877236
3502.997488	363905.361976	46.882241
3503.071839	363900.363416	46.887245
3503.106564	363904.937981	46.892250
3503.061158	363910.441190	46.897255
3503.259001	363903.158612	46.902260
3502.789692	363911.934753	46.907265
3503.360785	363899.275417	46.912269
3503.300048	363912.236076	46.917274
3502.763066	363915.679722	46.922279
3503.504706	363912.076853	46.927284
3503.022552	363924.544368	46.932289
3503.174502	363918.668455	46.937293
3503.529633	363936.117796	46.942298
3503.680692	363922.761558	46.947303
3503.670633	363918.234333	46.952308
3503.557436	363900.289099	46.957313
3503.500712	363880.044989	46.962317
3503.497248	363887.602517	46.967322
3503.598596	363882.701462	46.972327
3503.601061	363896.415448	46.977332
3503.600674	363886.696159	46.982337
3503.361019	363871.111734	46.987341
3503.120456	363866.366506	46.992346
3503.072680	363854.644642	46.997351
3503.371754	363871.237781	47.002356
3503.034464	363868.594237	47.007361
3503.368072	363859.356459	47.012365
3503.252784	363870.442913	47.017370
3503.195186	363872.971130	47.022375
3503.338298	363872.287142	47.027380
3503.376897	363869.100740	47.032385
3503.549552	363850.779526	47.037389
3503.046259	363821.471662	47.042394
3503.310500	363811.990403	47.047399
3503.454068	363813.138297	47.052404
3503.203449	363807.860333	47.057409
3503.210320	363816.790206	47.062413
3503.300111	363808.583273	47.067418
3503.133973	363810.925102	47.072423
3503.237547	363807.066885	47.077428
3503.260598	363808.513714	47.082433
3503.338190	363816.898086	47.087437
3503.299612	363810.161745	47.092442
3503.326644	363820.716835	47.097447
3503.505184	363777.078050	47.102452
3502.946610	363781.695536	47.107457
3503.502731	363765.858050	47.112461
3503.506706	363783.591959	47.117466
3503.176100	363773.975739	47.122471
3503.483781	363785.097121	47.127476
3503.358237	363786.491111	47.132481
3503.502978	363783.338811	47.137485
3503.401034	363766.638494	47.142490
3503.024055	363742.755594	47.147495
3503.087952	363739.717848	47.152500
3503.259849	363747.145900	47.157505
3503.127649	363738.439729	47.162509
3503.073817	363746.615896	47.167514
3503.215901	363744.965201	47.172519
3503.418457	363746.943419	47.177524
3503.129680	363735.768502	47.182529
3503.178877	363728.509396	47.187533
3503.296293	363751.619484	47.192538
3503.246285	363745.800921	47.197543
3503.465853	363743.450992	47.202548
3502.974861	363754.800421	47.207553
3503.104558	363755.517964	47.212557
3503.307565	363747.980106	47.217562
3503.188768	363746.090772	47.222567
3503.150712	363720.271434	47.227572
3503.010504	363719.912116	47.232577
3503.391181	363716.315410	47.237581
3503.228507	363715.934201	47.242586
3503.103500	363719.668945	47.247591
3503.434977	363716.181792	47.252596
3503.454348	363720.682472	47.257601
3503.402368	363722.268385	47.262605
3503.668852	363713.804507	47.267610
3503.329385	363719.506891	47.272615
3503.546159	363713.188157	47.277620
3503.433591	363693.029124	47.282625
3503.671181	363687.343194	47.287629
3503.577032	363691.632827	47.292634
3503.298270	363688.623805	47.297639
3503.478960	363683.990069	47.302644
3502.955678	363688.754649	47.307649
3503.386480	363671.028649	47.312653
3503.518557	363675.078969	47.317658
3503.330243	363654.881007	47.322663
3502.990359	363660.583464	47.327668
3503.118835	363656.212419	47.332673
3503.133331	363653.589579	47.337677
3503.146015	363662.544007	47.342682
3502.956023	363653.719736	47.347687
3503.296661	363647.076084	47.352692
3503.260049	363652.501602	47.357697
3503.228440	363659.809178	47.362701
3502.968345	363654.380031	47.367706
3503.322640	363663.000569	47.372711
3503.291832	363660.893770	47.377716
3503.081005	363660.927275	47.382721
3503.020358	363666.814581	47.387725
3503.240562	363666.652724	47.392730
3503.128147	363670.232819	47.397735
3503.611662	363664.737001	47.402740
3503.045433	363653.198825	47.407745
3502.919752	363637.138311	47.412749
3503.055212	363631.646627	47.417754
3502.804972	363630.210615	47.422759
3503.008291	363653.739719	47.427764
3502.914238	363664.822866	47.432769
3503.165206	363655.267342	47.437773
3503.366872	363667.423268	47.442778
3502.699444	363659.717678	47.447783
3503.250578	363660.266821	47.452788
3503.291150	363661.659997	47.457793
3502.950799	363640.315645	47.462797
3503.133839	363641.584523	47.467802
3503.093740	363635.891598	47.472807
3503.173623	363636.388023	47.477812
3502.788737	363648.458577	47.482817
3503.364494	363632.516165	47.487821
3503.360300	363645.595180	47.492826
3502.887390	363649.105048	47.497831
3503.470612	363647.715381	47.502836
3503.000102	363650.741434	47.507841
3503.618442	363644.715421	47.512845
3503.328504	363659.900564	47.517850
3503.195481	363649.286212	47.522855
3503.142073	363641.051001	47.527860
3502.924729	363657.267868	47.532865
3503.466363	363643.824358	47.537869
3503.216700	363643.406013	47.542874
3503.174518	363659.162641	47.547879
3503.051384	363652.490534	47.552884
3503.148646	363657.564115	47.557889
3503.425268	363631.847643	47.562893
3503.178934	363625.754774	47.567898
3503.162454	363619.600123	47.572903
3503.382487	363608.344736	47.577908
3502.999785	363625.936285	47.582913
3502.747936	363614.322954	47.587917
3503.057161	363619.948241	47.592922
3502.786952	363618.489942	47.597927
3503.053054	363621.959311	47.602932
3503.220892	363622.289167	47.607937
3503.039426	363628.933453	47.612941
3503.103846	363627.625803	47.617946
3503.645042	363624.309040	47.622951
3503.501785	363627.308803	47.627956
3503.012347	363628.734883	47.632961
3503.272498	363624.190355	47.637965
3503.395595	363628.598313	47.642970
3503.260532	363646.939466	47.647975
3503.196080	363635.881725	47.652980
3502.919953	363638.342726	47.657985
3503.607728	363622.993256	47.662989
3503.347303	363607.971792	47.667994
3503.422302	363596.942882	47.672999
3503.179444	363588.737612	47.678004
3503.222460	363593.997884	47.683009
3503.257242	363603.534040	47.688013
3503.642508	363592.354303	47.693018
3503.154678	363595.128659	47.698023
3503.247115	363599.312472	47.703028
3503.224869	363600.003151	47.708033
3503.653113	363596.246251	47.713037
3503.216788	363588.478670	47.718042
3503.088675	363578.626844	47.723047
3503.368116	363576.394662	47.728052
3502.980816	363582.028292	47.733057
3503.033278	363571.715371	47.738061
3503.602842	363576.510742	47.743066
3503.382213	363569.319713	47.748071
3503.532004	363580.593325	47.753076
3503.046957	363570.950590	47.758081
3503.261705	363572.748780	47.763085
3503.058247	363580.541528	47.768090
3503.129808	363574.093068	47.773095
3503.578663	363568.755383	47.778100
3502.992445	363557.856442	47.783105
3503.119911	363546.183126	47.788109
3503.525172	363536.246969	47.793114
3503.124338	363537.786264	47.798119
3503.111732	363539.009743	47.803124
3503.119181	363548.957335	47.808129
3503.277246	363542.647860	47.813133
3503.394274	363539.220040	47.818138
3503.293912	363549.769888	47.823143
3503.279198	363534.633223	47.828148
3502.962239	363539.034427	47.833153
3503.294088	363540.661442	47.838157
3503.463690	363538.319403	47.843162
3503.309379	363528.420820	47.848167
3503.116975	363506.849465	47.853172
3503.234086	363509.604521	47.858177
3503.240911	363499.680458	47.863181
3503.329366	363504.221125	47.868186
3503.193678	363517.829844	47.873191
3503.408207	363507.974723	47.878196
3503.069726	363507.137869	47.883201
3503.131693	363512.700483	47.888205
3503.065047	363510.014131	47.893210
3502.845799	363515.239542	47.898215
3503.373019	363505.971086	47.903220
3503.236697	363523.065731	47.908225
3503.282404	363505.324217	47.913229
3503.153382	363506.311662	47.918234
3502.979560	363519.035870	47.923239
3503.572069	363503.574201	47.928244
3503.204100	363498.212977	47.933249
3503.307134	363489.495014	47.938253
3503.575546	363478.740828	47.943258
3503.387917	363470.119700	47.948263
3503.857390	363480.223261	47.953268
3503.440761	363476.676252	47.958273
3503.452080	363491.483052	47.963277
3503.324193	363461.733949	47.968282
3502.974271	363463.723190	47.973287
3503.403597	363457.065490	47.978292
3503.385664	363448.697415	47.983297
3503.187379	363451.807665	47.988301
3503.190009	363447.609160	47.993306
3503.080043	363460.094293	47.998311
3503.274330	363448.105060	48.003316
3503.102758	363460.574488	48.008321
3503.231192	363448.697443	48.013325
3503.371351	363451.855964	48.018330
3503.039830	363454.351176	48.023335
3503.521023	363449.848017	48.028340
3503.417152	363447.421987	48.033345
3503.357643	363421.936646	48.038349
3503.386257	363411.169465	48.043354
3503.245535	363416.636914	48.048359
3503.492682	363405.300859	48.053364
3503.281869	363421.084228	48.058369
3503.374904	363410.484971	48.063373
3503.703320	363415.420260	48.068378
3503.105161	363407.474680	48.073383
3503.320181	363377.951197	48.078388
3502.907026	363388.067094	48.083393
3503.141443	363374.570299	48.088397
3503.212773	363376.671055	48.093402
3503.353244	363380.618297	48.098407
3503.584561	363370.556940	48.103412
3503.105923	363389.054288	48.108417
3503.311524	363385.154462	48.113421
3503.107119	363383.660308	48.118426
3502.979554	363386.225057	48.123431
3503.304211	363384.240157	48.128436
3502.951248	363382.006167	48.133441
3503.170583	363376.221308	48.138445
3503.553900	363383.132558	48.143450
3503.099072	363387.631905	48.148455
3503.293864	363368.569122	48.153460
3503.037698	363363.495536	48.158465
3503.294044	363357.145054	48.163469
3503.294174	363347.272905	48.168474
3502.947256	363342.188220	48.173479
3503.486174	363349.889086	48.178484
3503.323762	363350.372931	48.183489
3503.195868	363352.174411	48.188493
3503.463592	363351.292606	48.193498
3503.401985	363352.956386	48.198503
3503.452708	363352.846766	48.203508
3503.124013	363365.570056	48.208513
3503.073977	363352.856103	48.213517
3503.185091	363352.711491	48.218522
3503.030127	363349.479322	48.223527
3503.087622	363323.339327	48.228532
3503.324188	363340.018872	48.233537
3503.632061	363331.293939	48.238541
3503.504147	363330.601902	48.243546
3503.032388	363324.799073	48.248551
3503.357070	363330.345619	48.253556
3503.421141	363328.936240	48.258561
3503.387207	363325.888488	48.263565
3503.358246	363324.137599	48.268570
3503.250783	363314.536894	48.273575
3503.155869	363303.585664	48.278580
3502.954477	363299.419400	48.283585
3502.988209	363302.976418	48.288589
3503.172277	363295.746810	48.293594
3503.032508	363288.415732	48.298599
3502.921414	363288.102697	48.303604
3502.816985	363302.291753	48.308609
3502.840972	363324.399062	48.313613
3503.067754	363336.347553	48.318618
3503.088009	363331.306595	48.323623
3503.232510	363335.456757	48.328628
3503.130286	363339.366039	48.333633
3503.485863	363332.796313	48.338637
3503.204783	363306.175507	48.343642
3502.975469	363306.466377	48.348647
3503.593724	363297.412483	48.353652
3503.288218	363290.769155	48.358657
3503.145624	363303.488485	48.363661
3503.262683	363297.490788	48.368666
3503.169505	363304.095719	48.373671
3502.866040	363301.930232	48.378676
3503.277412	363304.180786	48.383681
3503.194552	363309.028441	48.388685
3503.085478	363301.870622	48.393690
3503.018907	363321.778611	48.398695
3503.478348	363302.292300	48.403700
3503.286554	363306.292078	48.408705
3503.390559	363308.718444	48.413709
3503.521000	363283.075776	48.418714
3503.420296	363277.112503	48.423719
3503.454723	363278.353998	48.428724
3503.134080	363274.461025	48.433729
3503.367493	363276.994156	48.438733
3503.281760	363277.364102	48.443738
3503.065938	363280.553469	48.448743
3503.836576	363282.212900	48.453748
3503.347869	363262.978244	48.458753
3503.379839	363244.602699	48.463757
3503.181894	363246.567922	48.468762
3502.920430	363241.953155	48.473767
3503.238421	363240.605407	48.478772
3503.200052	363250.585751	48.483777
3503.510594	363240.969835	48.488781
3503.263977	363240.983555	48.493786
3503.062558	363247.580161	48.498791
3503.581289	363240.450301	48.503796
3503.650403	363245.910041	48.508801
3503.115368	363225.588596	48.513805
3503.238517	363208.470829	48.518810
3502.990691	363210.316719	48.523815
3503.343486	363206.698937	48.528820
3502.822726	363219.630741	48.533825
3503.302007	363205.408192	48.538829
3503.031243	363211.099777	48.543834
3502.687839	363215.199863	48.548839
3502.783706	363213.556457	48.553844
3502.694257	363226.496404	48.558849
3503.166140	363239.881932	48.563853
3503.713222	363247.199862	48.568858
3503.318066	363233.828001	48.573863
3503.328821	363217.949325	48.578868
3503.298350	363227.317766	48.583873
3503.551443	363215.802615	48.588877
3503.534465	363206.620133	48.593882
3503.367962	363220.869916	48.598887
3503.595187	363206.916214	48.603892
3503.593901	363190.988544	48.608897
3503.621518	363179.839805	48.613901
3503.422581	363186.461472	48.618906
3503.284439	363186.127268	48.623911
3503.253352	363174.351704	48.628916
3503.408150	363180.561230	48.633921
3503.291401	363166.738228	48.638925
3503.320179	363156.352626	48.643930
3503.013288	363147.394074	48.648935
3503.108423	363130.458816	48.653940
3503.084089	363141.251180	48.658945
3503.238665	363148.427625	48.663949
3503.287732	363137.580815	48.668954
3503.167852	363148.057508	48.673959
3503.207542	363143.217011	48.678964
3502.848281	363156.835738	48.683969
3503.158482	363151.519925	48.688973
3503.495772	363141.747094	48.693978
3503.136258	363155.747524	48.698983
3503.262676	363146.924023	48.703988
3503.289994	363150.736508	48.708993
3503.158729	363150.706547	48.713997
3503.197694	363150.751451	48.719002
3502.867550	363157.470197	48.724007
3503.480919	363158.340282	48.729012
3503.245605	363153.212488	48.734017
3503.123680	363132.723916	48.739021
3503.291174	363122.850704	48.744026
3503.168090	363134.396563	48.749031
3503.361661	363113.400109	48.754036
3503.250161	363123.163044	48.759041
3503.393042	363115.889031	48.764045
3503.143944	363127.861920	48.769050
3503.028883	363119.051145	48.774055
3503.154956	363121.474034	48.779060
3502.915418	363133.470855	48.784065
3502.992335	363137.199167	48.789069
3503.245482	363121.816466	48.794074
3503.071531	363130.953168	48.799079
3503.456672	363126.897715	48.804084
3503.316570	363125.749606	48.809089
3503.486203	363132.821896	48.814093
3503.246108	363128.000186	48.819098
3503.004980	363105.189579	48.824103
3503.607424	363099.903891	48.829108
3503.280352	363108.276034	48.834113
3503.391794	363096.910469	48.839117
3503.661609	363100.430179	48.844122
3503.057642	363094.978997	48.849127
3503.392925	363110.956024	48.854132
3503.523990	363102.030003	48.859137
3503.260106	363092.250426	48.864141
3503.115229	363074.996873	48.869146
3503.148425	363057.918716	48.874151
3503.255415	363059.606741	48.879156
3502.931886	363065.764682	48.884161
3503.034403	363057.199385	48.889165
3503.058963	363065.821275	48.894170
3503.323306	363061.861246	48.899175
3502.999133	363063.948210	48.904180
3502.955846	363071.919275	48.909185
3503.346439	363057.710703	48.914189
3503.547388	363060.859640	48.919194
3503.215457	363068.392898	48.924199
3503.580273	363050.346318	48.929204
3503.271414	363068.969619	48.934209
3503.380128	363066.153741	48.939213
3503.370925	363063.483726	48.944218
3503.064748	363042.718912	48.949223
3503.519199	363040.255482	48.954228
3503.180848	363027.866906	48.959233
3503.539949	363040.557883	48.964237
3503.668513	363032.268350	48.969242
3503.496911	363044.152677	48.974247
3503.516633	363020.995459	48.979252
3503.205801	363007.915532	48.984257
3503.109454	362994.089254	48.989261
3503.228677	362994.274135	48.994266
3503.377630	362994.199873	48.999271
3503.606606	362988.947771	49.004276
3502.911401	362996.207696	49.009281
3503.536996	362996.846853	49.014285
3503.590383	362990.808294	49.019290
3503.175808	362989.830795	49.024295
3503.266263	362993.862310	49.029300
3503.200921	362987.308191	49.034305
3503.199152	362971.482299	49.039309
3503.234074	362967.558533	49.044314
3503.076790	362965.319031	49.049319
3503.362497	362968.098355	49.054324
3503.410500	362956.971783	49.059329
3503.042612	362970.413818	49.064333
3503.356239	362959.906806	49.069338
3503.044880	362960.872200	49.074343
3503.301821	362964.343067	49.079348
3503.009154	362967.264716	49.084353
3503.090580	362959.745951	49.089357
3503.324570	362963.296780	49.094362
3503.489074	362973.092445	49.099367
3503.537393	362958.963398	49.104372
3502.950287	362940.583827	49.109377
3503.141726	362928.493133	49.114381
3503.369845	362921.383724	49.119386
3503.100244	362936.667666	49.124391
3503.081362	362925.322662	49.129396
3503.325312	362925.767712	49.134401
3503.198704	362926.882009	49.139405
3503.388953	362922.272130	49.144410
3502.946374	362922.723939	49.149415
3503.323110	362917.524802	49.154420
3503.269318	362930.688193	49.159425
3503.428565	362921.325128	49.164429
3503.485047	362921.952482	49.169434
3503.101395	362918.909103	49.174439
3503.204729	362904.058901	49.179444
3503.347082	362898.845928	49.184449
3503.283171	362886.337594	49.189453
3503.137307	362900.227991	49.194458
3503.133070	362896.971962	49.199463
3503.043592	362891.032309	49.204468
3503.135223	362905.266823	49.209473
3502.815820	362906.437044	49.214477
3503.494936	362895.999458	49.219482
3503.277856	362909.926556	49.224487
3503.138227	362907.429817	49.229492
3503.280313	362908.298081	49.234497
3503.557619	362900.468451	49.239501
3503.357351	362912.891675	49.244506
3503.020932	362903.886855	49.249511
3503.243349	362897.847006	49.254516
3503.557493	362887.187230	49.259521
3503.408317	362876.448032	49.264525
3503.440066	362874.178642	49.269530
3503.079774	362872.327451	49.274535
3503.287290	362874.355811	49.279540
3503.396275	362876.806858	49.284545
3503.320445	362875.419582	49.289549
3503.369697	362876.277078	49.294554
3503.252152	362880.061599	49.299559
3503.669395	362844.399164	49.304564
3503.409360	362858.434845	49.309569
3503.082217	362840.421245	49.314573
3503.340421	362841.347486	49.319578
3502.953199	362842.452097	49.324583
3502.974076	362833.314445	49.329588
3502.813165	362836.571493	49.334593
3503.073284	362840.270867	49.339597
3503.072148	362845.563649	49.344602
3502.871605	362847.681966	49.349607
3503.040992	362838.724391	49.354612
3502.797258	362850.772837	49.359617
3502.921187	362843.196445	49.364621
3503.264898	362840.725068	49.369626
3502.990278	362854.152392	49.374631
3502.690353	362841.579581	49.379636
3502.947992	362854.083094	49.384641
3502.876742	362855.850194	49.389645
3502.956429	362870.519161	49.394650
3503.055098	362874.091390	49.399655
3503.245696	362884.722612	49.404660
3503.155805	362890.131198	49.409665
3502.946346	362881.157191	49.414669
3503.077681	362865.513776	49.419674
3502.968606	362873.495275	49.424679
3503.146695	362875.324733	49.429684
3503.174819	362862.776399	49.434689
3503.038411	362862.340141	49.439693
3503.035448	362866.615435	49.444698
3502.925976	362865.106256	49.449703
3503.534257	362867.376591	49.454708
3503.326273	362865.628542	49.459713
3502.896215	362866.663592	49.464717
3503.104920	362852.381935	49.469722
3503.114089	362858.461861	49.474727
3503.089309	362856.684849	49.479732
3503.081229	362858.620072	49.484737
3503.492373	362853.644488	49.489741
3503.423317	362862.179439	49.494746
3503.170096	362860.845652	49.499751
3503.663379	362859.470180	49.504756
3503.353844	362870.918359	49.509761
3503.707970	362846.359638	49.514765
3503.485346	362829.576283	49.519770
3503.239680	362829.411741	49.524775
3503.025307	362826.621482	49.529780
3502.821005	362818.664423	49.534785
3502.924717	362822.795635	49.539789
3503.184635	362826.800374	49.544794
3502.770757	362823.507323	49.549799
3503.200189	362809.114425	49.554804
3502.790556	362815.158789	49.559809
3503.192812	362821.125687	49.564813
3503.234900	362828.421743	49.569818
3503.156851	362827.874481	49.574823
3503.177075	362828.558457	49.579828
3503.211748	362824.380274	49.584833
3503.174945	362831.358024	49.589837
3503.465125	362832.406432	49.594842
3502.947219	362835.338254	49.599847
3503.218111	362821.453865	49.604852
3502.899582	362830.130040	49.609857
3502.985455	362843.627597	49.614861
3503.176101	362833.368998	49.619866
3503.175241	362833.827307	49.624871
3503.175137	362833.140501	49.629876
3502.819792	362846.504256	49.634881
3503.230714	362839.340490	49.639885
3503.631065	362840.625924	49.644890
3503.323477	362840.293061	49.649895
3503.370599	362804.638220	49.654900
3503.190605	362807.160400	49.659905
3503.137077	362793.429070	49.664909
3502.915081	362792.726454	49.669914
3503.335638	362799.352016	49.674919
3502.985415	362789.815024	49.679924
3502.973150	362813.862082	49.684929
3502.951501	362802.924596	49.689933
3503.032515	362815.583264	49.694938
3502.725842	362812.604041	49.699943
3503.272616	362802.721689	49.704948
3503.037014	362813.801972	49.709953
3502.911856	362805.781510	49.714957
3503.009287	362807.445611	49.719962
3502.515331	362819.508179	49.724967
3503.420985	362827.278377	49.729972
3503.329237	362849.378765	49.734977
3503.338827	362833.372920	49.739981
3503.761118	362818.446821	49.744986
3503.090694	362829.163289	49.749991
3503.158857	362819.661937	49.754996
3503.244266	362820.615496	49.760001
3502.829633	362812.157355	49.765005
3503.105310	362815.625272	49.770010
3503.214132	362823.368778	49.775015
3503.231614	362813.697326	49.780020
3503.033323	362818.079838	49.785025
3503.335572	362829.227754	49.790029
3503.333819	362828.515764	49.795034
3503.246379	362824.534996	49.800039
3503.520565	362814.492185	49.805044
3503.358428	362801.312360	49.810049
3503.354938	362789.354224	49.815053
3503.311497	362779.895953	49.820058
3503.130690	362784.911813	49.825063
3503.142861	362775.088528	49.830068
3503.216665	362790.470894	49.835073
3503.108461	362782.625858	49.840077
3503.158263	362786.434819	49.845082
3503.158612	362785.060941	49.850087
3502.997009	362774.858017	49.855092
3502.985210	362786.844368	49.860097
3502.975201	362785.395795	49.865101
3503.346557	362780.146605	49.870106
3503.265484	362787.334917	49.875111
3503.168245	362784.322582	49.880116
3502.989124	362788.676622	49.885121
3503.425014	362787.208444	49.890125
3503.606906	362778.859546	49.895130
3503.447504	362774.152264	49.900135
3503.574267	362750.927100	49.905140
3503.490493	362749.591966	49.910145
3503.187998	362752.896848	49.915149
3503.483649	362749.440732	49.920154
3503.306751	362764.302963	49.925159
3503.483649	362746.489530	49.930164
3503.079797	362728.004569	49.935169
3503.146145	362724.406591	49.940173
3503.410299	362706.223126	49.945178
3503.272423	362721.257313	49.950183
3503.156644	362712.904575	49.955188
3503.353049	362730.506688	49.960193
3503.541415	362719.917647	49.965197
3503.322220	362715.601478	49.970202
3503.176528	362728.601344	49.975207
3503.701226	362714.320578	49.980212
3503.288586	362694.641105	49.985217
3503.445701	362685.354663	49.990221
3503.530890	362677.809813	49.995226
3503.140963	362689.321635	50.000231
3503.290484	362673.878835	50.005236
3502.953101	362682.736128	50.010241
3502.995956	362671.839303	50.015245
3503.692938	362665.240954	50.020250
3503.155963	362683.188027	50.025255
3503.382019	362666.588125	50.030260
3503.279909	362658.971105	50.035265
3503.232397	362650.633007	50.040269
3503.343868	362631.023316	50.045274
3503.066410	362636.766918	50.050279
3503.341549	362637.894041	50.055284
3503.288209	362641.541209	50.060289
3503.342032	362641.151208	50.065293
3503.352556	362648.961171	50.070298
3503.251763	362641.242163	50.075303
3503.606803	362638.005649	50.080308
3502.913996	362639.743799	50.085313
3503.160125	362649.501183	50.090317
3503.458838	362646.451687	50.095322
3503.093076	362633.965561	50.100327
3503.029748	362618.683616	50.105332
3502.989732	362619.173562	50.110337
3503.139152	362619.022893	50.115341
3503.255391	362610.480788	50.120346
3502.644732	362623.376081	50.125351
3503.335675	362615.201121	50.130356
3502.912449	362612.825535	50.135361
3502.944384	362619.105449	50.140365
3503.108577	362621.802226	50.145370
3503.142289	362622.865740	50.150375
3503.507079	362609.271778	50.155380
3503.182042	362620.239024	50.160385
3503.250099	362602.697187	50.165389
3503.180950	362622.096994	50.170394
3502.891460	362617.054039	50.175399
3503.236922	362620.129270	50.180404
3502.994538	362616.885426	50.185409
3503.108966	362628.750084	50.190413
3503.190144	362617.821743	50.195418
3502.949056	362615.137472	50.200423
3503.055392	362611.507719	50.205428
3502.919894	362627.355785	50.210433
3503.259225	362624.579755	50.215437
3503.482706	362621.974706	50.220442
3503.195033	362628.686815	50.225447
3503.826054	362623.625556	50.230452
3503.448733	362614.143702	50.235457
3503.308400	362582.436777	50.240461
3503.577594	362580.587834	50.245466
3503.404056	362587.205571	50.250471
3503.405475	362576.009940	50.255476
3503.169915	362582.612038	50.260481
3503.520078	362588.027422	50.265485
3503.564594	362580.921544	50.270490
3503.276750	362570.229643	50.275495
3503.172187	362557.498647	50.280500
3503.322381	362549.867166	50.285505
3503.051453	362558.332309	50.290509
3503.139689	362544.909272	50.295514
3503.268676	362559.316098	50.300519
3503.395726	362544.487477	50.305524
3503.071862	362554.309549	50.310529
3503.366967	362552.939955	50.315533
3503.966016	362547.120407	50.320538
3503.336750	362539.001483	50.325543
3503.213521	362510.396037	50.330548
3503.399939	362514.743202	50.335553
3503.557855	362514.336744	50.340557
3503.733654	362511.433893	50.345562
3503.410241	362511.739643	50.350567
3503.559675	362497.060135	50.355572
3503.152282	362501.602957	50.360577
3503.180567	362478.087892	50.365581
3503.202865	362480.043773	50.370586
3503.191361	362480.859993	50.375591
3503.167438	362474.630032	50.380596
3503.453271	362481.633163	50.385601
3503.147501	362477.915883	50.390605
3503.197530	362488.951087	50.395610
3503.305416	362476.033815	50.400615
3503.573989	362475.126416	50.405620
3503.026903	362484.424012	50.410625
3502.987865	362482.801907	50.415629
3503.595805	362486.217320	50.420634
3502.975079	362479.038484	50.425639
3503.063362	362466.175197	50.430644
3503.561004	362456.300539	50.435649
3503.376195	362447.195329	50.440653
3503.221242	362442.054751	50.445658
3503.079388	362441.670239	50.450663
3503.445981	362427.236268	50.455668
3502.949973	362443.039612	50.460673
3502.900955	362448.340009	50.465677
3503.376526	362444.779092	50.470682
3503.305266	362445.299425	50.475687
3503.577318	362441.643460	50.480692
3503.249506	362445.461258	50.485697
3502.964128	362446.804223	50.490701
3503.428459	362440.089955	50.495706
3502.930742	362442.713274	50.500711
3503.684336	362420.355743	50.505716
3503.224167	362430.428391	50.510721
3503.006869	362414.407382	50.515725
3503.375858	362409.591083	50.520730
3502.815661	362404.692680	50.525735
3502.915409	362384.550402	50.530740
3502.816943	362362.581994	50.535745
3502.666152	362315.813321	50.540749
3503.109801	362265.999042	50.545754
3502.504513	362220.294469	50.550759
3502.232214	362145.682879	50.555764
3502.290883	362072.978095	50.560769
3501.960839	362005.118277	50.565773
3501.959851	361914.305964	50.570778
3501.320754	361824.586708	50.575783
3500.898441	361721.805185	50.580788
3500.549034	361629.673376	50.585793
3500.331264	361513.449533	50.590797
3500.229544	361403.059440	50.595802
3499.657790	361286.382097	50.600807
3499.558892	361150.901989	50.605812
3499.087602	361022.045267	50.610817
3498.657793	360888.372452	50.615821
3498.078938	360744.620964	50.620826
3497.477625	360605.885369	50.625831
3497.127836	360461.995031	50.630836
3496.658819	360315.832994	50.635841
3496.267725	360161.362858	50.640845
3495.918102	360006.503979	50.645850
3495.001336	359855.016795	50.650855
3494.660205	359683.513865	50.655860
3494.084449	359528.790983	50.660865
3493.705425	359359.201352	50.665869
3492.787452	359188.754819	50.670874
3492.194982	359017.111136	50.675879
3492.139173	358850.420409	50.680884
3491.242550	358682.335247	50.685889
3490.862407	358512.564711	50.690893
3490.375867	358325.506604	50.695898
3489.595323	358149.970801	50.700903
3489.448626	357957.004780	50.705908
3488.968178	357777.755840	50.710913
3488.121821	357580.852880	50.715917
3487.634673	357392.213597	50.720922
3487.039951	357200.689605	50.725927
3486.674894	357002.410437	50.730932
3485.743803	356807.146438	50.735937
3485.147619	356608.393292	50.740941
3484.290666	356423.804087	50.745946
3483.457344	356234.324479	50.750951
3482.998791	356023.205048	50.755956
3482.003137	355840.035264	50.760961
3481.237450	355645.860309	50.765965
3481.192132	355462.666147	50.770970
3480.628758	355262.172022	50.775975
3480.139515	355054.056304	50.780980
3479.184775	354863.801860	50.785985
3478.617362	354675.750397	50.790989
3478.376524	354467.160389	50.795994
3477.589668	354261.582476	50.800999
3477.083813	354043.972868	50.806004
3476.032197	353844.135713	50.811009
3475.406566	353640.260371	50.816013
3474.864246	353436.294708	50.821018
3473.893383	353240.896079	50.826023
3473.697408	353034.354601	50.831028
3472.898001	352834.600940	50.836033
3472.029423	352622.361686	50.841037
3471.376999	352414.973750	50.846042
3470.456014	352223.508152	50.851047
3469.989247	352014.206000	50.856052
3469.381646	351823.427455	50.861057
3468.541573	351613.444695	50.866061
3468.319507	351418.709875	50.871066
3467.599898	351210.360746	50.876071
3466.878101	350992.721752	50.881076
3465.969229	350792.417803	50.886081
3465.568256	350591.294738	50.891085
3465.147874	350381.113544	50.896090
3463.986291	350184.104984	50.901095
3463.556187	349972.269441	50.906100
3462.827684	349764.832373	50.911105
3461.912871	349567.273545	50.916109
3461.550656	349364.205531	50.921114
3460.570540	349160.929049	50.926119
3460.119061	348946.191471	50.931124
3459.379821	348751.274344	50.936129
3458.527941	348544.793884	50.941133
3458.383865	348337.869873	50.946138
3457.286344	348136.593420	50.951143
3456.524096	347925.489726	50.956148
3455.626822	347724.765521	50.961153
3455.101541	347519.731294	50.966157
3454.226279	347323.507184	50.971162
3453.812372	347128.812932	50.976167
3453.008507	346927.205744	50.981172
3452.164072	346729.065777	50.986177
3451.337233	346529.497000	50.991181
3451.064366	346337.399341	50.996186
3450.108934	346142.889152	51.001191
3449.652171	345941.274504	51.006196
3448.840167	345747.631143	51.011201
3448.385179	345545.225792	51.016205
3447.792782	345351.775458	51.021210
3446.764365	345154.397290	51.026215
3446.227968	344951.773664	51.031220
3445.688375	344757.778491	51.036225
3444.890062	344551.631437	51.041229
3444.727781	344352.790037	51.046234
3443.848303	344158.032115	51.051239
3443.122729	343955.816767	51.056244
3442.513078	343760.811243	51.061249
3441.884117	343555.346636	51.066253
3441.130997	343360.209762	51.071258
3440.228126	343157.434295	51.076263
3440.010908	342950.426175	51.081268
3439.010684	342758.355441	51.086273
3438.100453	342561.713566	51.091277
3437.481042	342356.319706	51.096282
3436.563852	342145.652275	51.101287
3436.280354	341950.818396	51.106292
3435.673800	341760.005882	51.111297
3434.965345	341560.936140	51.116301
3434.598127	341354.888121	51.121306
3434.057980	341159.303212	51.126311
3433.504383	340948.166896	51.131316
3432.553381	340749.692894	51.136321
3431.669296	340549.451280	51.141325
3430.913226	340345.650521	51.146330
3430.176665	340150.755327	51.151335
3429.547868	339950.827801	51.156340
3428.627745	339754.789461	51.161345
3428.291487	339566.803922	51.166349
3427.956480	339359.904194	51.171354
3426.778941	339177.548916	51.176359
3426.316814	338972.246272	51.181364
3425.334833	338779.193011	51.186369
3424.818075	338581.025354	51.191373
3424.360392	338377.196537	51.196378
3423.588894	338195.588846	51.201383
3422.929144	337990.925258	51.206388
3421.927427	337796.930302	51.211393
3421.751899	337589.872376	51.216397
3420.914835	337396.053839	51.221402
3419.953239	337206.225611	51.226407
3419.647009	337002.419451	51.231412
3418.887756	336811.132527	51.236417
3417.892201	336619.831502	51.241421
3417.495586	336416.190567	51.246426
3417.140066	336215.215466	51.251431
3416.263658	336021.806429	51.256436
3415.118736	335825.511752	51.261441
3414.669664	335618.159976	51.266445
3414.272893	335433.685162	51.271450
3413.436657	335247.522798	51.276455
3412.929948	335036.741645	51.281460
3412.113159	334848.233051	51.286465
3411.523154	334648.945087	51.291469
3410.861809	334456.897724	51.296474
3410.127893	334269.545473	51.301479
3409.037466	334068.934799	51.306484
3408.118831	333881.610705	51.311489
3408.100700	333692.667161	51.316493
3407.755077	333496.290315	51.321498
3406.584433	333305.058571	51.326503
3406.111263	333104.653003	51.331508
3405.454069	332914.560979	51.336513
3405.016159	332726.292203	51.341517
3404.352297	332531.184971	51.346522
3403.688186	332328.898041	51.351527
3403.063815	332127.546208	51.356532
3401.822039	331934.489016	51.361537
3401.310889	331743.759770	51.366541
3400.725419	331553.449107	51.371546
3399.703819	331365.294508	51.376551
3399.281985	331176.026233	51.381556
3398.548265	330986.603117	51.386561
3397.608826	330793.113190	51.391565
3397.196499	330604.580232	51.396570
3396.259770	330415.824213	51.401575
3395.839742	330220.061178	51.406580
3395.173517	330029.250140	51.411585
3394.464915	329848.450714	51.416589
3393.885844	329665.517260	51.421594
3393.340095	329474.329322	51.426599
3392.917127	329279.888158	51.431604
3392.124379	329082.908122	51.436609
3391.349118	328894.733744	51.441613
3390.487343	328710.340574	51.446618
3390.153890	328503.815497	51.451623
3389.194275	328307.598164	51.456628
3388.712069	328136.764443	51.461633
3387.900317	327937.111192	51.466637
3387.470811	327738.746343	51.471642
3386.338896	327553.425645	51.476647
3385.953842	327372.798308	51.481652
3385.236348	327182.242839	51.486657
3384.728288	326988.216687	51.491661
3384.216513	326785.330548	51.496666
3383.297511	326595.085583	51.501671
3382.580860	326410.842220	51.506676
3382.176171	326220.285880	51.511681
3381.325101	326038.685318	51.516685
3380.912774	325838.912652	51.521690
3379.949015	325647.832315	51.526695
3379.614997	325452.934706	51.531700
3378.636670	325259.997142	51.536705
3377.777338	325073.940122	51.541709
3377.283138	324883.547544	51.546714
3376.652997	324694.321755	51.551719
3376.135140	324496.930327	51.556724
3374.790808	324313.494362	51.561729
3374.371436	324126.958249	51.566733
3373.999249	323938.250075	51.571738
3373.074886	323754.364546	51.576743
3372.149639	323561.745612	51.581748
3371.828996	323384.434592	51.586753
3370.719217	323189.119652	51.591757
3370.402416	323010.406877	51.596762
3369.722384	322826.888068	51.601767
3369.412982	322631.929035	51.606772
3368.416205	322455.104931	51.611777
3367.680415	322267.239846	51.616781
3367.389602	322072.480298	51.621786
3366.932713	321891.164818	51.626791
3366.118950	321696.690827	51.631796
3365.227991	321510.809193	51.636801
3364.175834	321321.540789	51.641805
3364.050876	321140.782344	51.646810
3363.243537	320956.770490	51.651815
3362.804150	320758.415949	51.656820
3361.783453	320572.552865	51.661825
3360.886791	320386.542470	51.666829
3361.053477	320193.004990	51.671834
3359.866393	320005.970336	51.676839
3359.077700	319824.626735	51.681844
3358.372818	319641.690862	51.686849
3357.729665	319443.365664	51.691853
3357.415947	319248.705433	51.696858
3356.458771	319074.414591	51.701863
3355.692941	318883.669911	51.706868
3355.031089	318714.958879	51.711873
3354.445869	318523.395562	51.716877
3353.882791	318337.353727	51.721882
3353.060291	318158.151069	51.726887
3352.219896	317961.967314	51.731892
3352.041271	317773.088138	51.736897
3351.351431	317589.483843	51.741901
3350.779382	317394.376844	51.746906
3349.861798	317211.215251	51.751911
3349.608282	317018.628863	51.756916
3348.999283	316837.938589	51.761921
3347.723756	316644.596435	51.766925
3347.490594	316451.420061	51.771930
3346.858279	316261.973125	51.776935
3346.263522	316071.068488	51.781940
3345.545797	315896.377523	51.786945
3344.813590	315699.535527	51.791949
3344.239475	315500.682005	51.796954
3343.224272	315317.455954	51.801959
3342.598989	315129.991907	51.806964
3341.810585	314942.094972	51.811969
3340.975329	314759.043164	51.816973
3340.760905	314572.786289	51.821978
3339.836328	314388.372920	51.826983
3339.361382	314196.172633	51.831988
3338.299308	314019.139341	51.836993
3337.678236	313825.968403	51.841997
3337.181482	313642.886558	51.847002
3336.289398	313461.572996	51.852007
3335.956547	313279.635935	51.857012
3335.066303	313086.098801	51.862017
3334.409744	312901.996940	51.867021
3333.781904	312724.154358	51.872026
3332.722207	312537.925737	51.877031
3332.305142	312358.241275	51.882036
3331.616133	312188.683310	51.887041
3330.752861	312008.508639	51.892045
3330.456787	311819.382430	51.897050
3329.407159	311648.811180	51.902055
3328.933329	311451.844018	51.907060
3328.451768	311286.122433	51.912065
3327.703201	311095.971605	51.917069
3327.005675	310914.164704	51.922074
3326.244424	310741.356532	51.927079
3326.017231	310560.646040	51.932084
3325.134934	310381.643143	51.937089
3324.771537	310188.094037	51.942093
3324.208758	309997.428177	51.947098
3323.325973	309828.635804	51.952103
3322.783974	309628.544148	51.957108
3321.977310	309447.108714	51.962113
3321.257276	309257.255936	51.967117
3320.664051	309078.103472	51.972122
3320.048953	308890.525345	51.977127
3319.472569	308696.574587	51.982132
3318.846416	308518.827069	51.987137
3317.785283	308329.943521	51.992141
3317.454933	308138.015620	51.997146
3316.379465	307962.681144	52.002151
3315.608950	307767.486373	52.007156
3315.377665	307593.647615	52.012161
3314.485803	307417.926821	52.017165
3313.696194	307229.635283	52.022170
3313.322067	307048.000561	52.027175
3312.389739	306868.109114	52.032180
3311.836045	306688.972413	52.037185
3311.023420	306505.980229	52.042189
3310.666862	306312.856837	52.047194
3309.961913	306145.610162	52.052199
3309.417758	305962.116373	52.057204
3308.481013	305769.440469	52.062209
3307.804778	305597.757571	52.067213
3307.203060	305410.172183	52.072218
3306.258049	305234.456850	52.077223
3305.866566	305035.072602	52.082228
3305.166199	304861.559062	52.087233
3304.407648	304676.696823	52.092237
3303.971826	304493.489490	52.097242
3303.098419	304323.949826	52.102247
3302.483319	304139.675359	52.107252
3301.464779	303962.060104	52.112257
3301.072110	303775.840044	52.117261
3300.679500	303600.238990	52.122266
3299.874377	303419.227807	52.127271
3299.057955	303230.782136	52.132276
3298.305153	303047.979598	52.137281
3298.220843	302883.915913	52.142285
3297.190310	302693.669866	52.147290
3296.598535	302512.521947	52.152295
3295.969482	302329.291485	52.157300
3295.472453	302144.410086	52.162305
3294.451552	301971.096552	52.167309
3293.942261	301778.984264	52.172314
3293.208260	301601.754071	52.177319
3292.747423	301417.477253	52.182324
3292.087713	301239.165311	52.187329
3291.208296	301051.159798	52.192333
3290.963322	300864.785413	52.197338
3290.011365	300682.164328	52.202343
3289.268105	300501.369066	52.207348
3288.793230	300336.498579	52.212353
3287.898638	300137.518371	52.217357
3287.318340	299951.654364	52.222362
3286.575214	299782.649251	52.227367
3285.918909	299598.604988	52.232372
3285.260713	299416.801877	52.237377
3284.274461	299237.724452	52.242381
3284.019415	299051.527858	52.247386
3283.126359	298875.465833	52.252391
3282.442922	298694.149806	52.257396
3281.897847	298513.524768	52.262401
3280.802904	298334.820128	52.267405
3280.338400	298164.368665	52.272410
3279.518060	297990.891849	52.277415
3279.388539	297806.584073	52.282420
3278.591249	297630.938586	52.287425
3277.608250	297458.352857	52.292429
3277.320896	297273.280033	52.297434
3276.642022	297105.255363	52.302439
3275.522546	296916.570183	52.307444
3274.946571	296746.924497	52.312449
3274.332715	296576.749845	52.317453
3273.784726	296398.084120	52.322458
3273.179506	296218.612338	52.327463
3272.766332	296028.999603	52.332468
3271.737544	295861.640394	52.337473
3270.743953	295683.783045	52.342477
3270.803251	295504.944032	52.347482
3269.976073	295323.672913	52.352487
3269.046802	295136.534873	52.357492
3268.433259	294969.083762	52.362497
3267.668607	294787.547603	52.367501
3267.340918	294614.524607	52.372506
3265.969123	294442.456120	52.377511
3265.677202	294264.359200	52.382516
3265.048151	294090.211953	52.387521
3264.518961	293920.913019	52.392525
3263.939569	293742.682871	52.397530
3263.154893	293568.865431	52.402535
3262.544023	293393.008440	52.407540
3261.818791	293207.211662	52.412545
3261.354489	293030.287038	52.417549
3260.646540	292839.724824	52.422554
3259.784399	292673.762908	52.427559
3259.333038	292492.353556	52.432564
3258.639548	292322.086180	52.437569
3257.654140	292143.333256	52.442573
3257.188711	291954.922160	52.447578
3256.533673	291790.633185	52.452583
3255.958404	291613.775986	52.457588
3254.955618	291436.833486	52.462593
3254.554063	291266.875733	52.467597
3253.991904	291092.206301	52.472602
3252.976473	290908.007168	52.477607
3252.437178	290733.333875	52.482612
3252.144222	290550.573719	52.487617
3250.988644	290382.950353	52.492621
3250.399722	290204.158798	52.497626
3249.915622	290027.719038	52.502631
3249.380818	289848.154657	52.507636
3248.551282	289670.062979	52.512641
3247.961376	289495.931713	52.517645
3247.611315	289309.690679	52.522650
3246.782466	289134.985767	52.527655
3245.628791	288957.632552	52.532660
3245.353813	288785.437522	52.537665
3244.405437	288619.996026	52.542669
3243.612305	288439.682133	52.547674
3242.950906	288263.116534	52.552679
3242.477771	288087.743508	52.557684
3241.502766	287921.134327	52.562689
3240.676279	287745.434994	52.567693
3240.413472	287568.041912	52.572698
3239.484713	287400.635641	52.577703
3238.873402	287235.089158	52.582708
3238.233114	287064.351718	52.587713
3237.611525	286891.726605	52.592717
3237.038334	286721.946161	52.597722
3236.386680	286559.003467	52.602727
3235.704977	286378.645346	52.607732
3234.845903	286205.802790	52.612737
3234.385212	286042.473099	52.617741
3233.996198	285862.450439	52.622746
3233.326372	285696.224860	52.627751
3232.376951	285519.295927	52.632756
3231.842438	285357.047279	52.637761
3231.006591	285178.011843	52.642765
3230.466717	285002.495034	52.647770
3229.731221	284837.603826	52.652775
3229.006261	284662.421772	52.657780
3228.323573	284495.586500	52.662785
3227.652041	284326.329927	52.667789
3227.258301	284139.660072	52.672794
3226.560400	283983.931119	52.677799
3225.940759	283806.567271	52.682804
3224.959487	283638.963939	52.687809
3224.175446	283465.853687	52.692813
3223.654010	283293.924299	52.697818
3222.748086	283135.553822	52.702823
3222.506702	282958.511843	52.707828
3221.635928	282792.215089	52.712833
3220.957367	282630.523088	52.717837
3220.710393	282450.629383	52.722842
3220.028584	282286.314566	52.727847
3219.425954	282114.703259	52.732852
3218.546667	281936.794079	52.737857
3217.833824	281753.433775	52.742861
3217.010370	281579.692449	52.747866
3216.227676	281420.359666	52.752871
3215.837858	281244.181093	52.757876
3215.112215	281074.575484	52.762881
3214.454116	280906.487244	52.767885
3214.129012	280739.263138	52.772890
3212.951428	280566.519905	52.777895
3212.620501	280394.279386	52.782900
3212.086571	280227.521165	52.787905
3211.004355	280050.662329	52.792909
3210.474186	279877.587298	52.797914
3209.798729	279710.036377	52.802919
3209.176818	279540.031992	52.807924
3208.529327	279364.734209	52.812929
3207.457603	279202.237684	52.817933
3207.139680	279039.902020	52.822938
3206.449839	278858.931407	52.827943
3206.125826	278685.059491	52.832948
3205.210486	278517.877409	52.837953
3204.329717	278341.750441	52.842957
3204.018496	278179.973896	52.847962
3203.443138	278015.004640	52.852967
3202.516703	277832.568674	52.857972
3201.945658	277667.369480	52.862977
3200.987034	277506.663088	52.867981
3200.558536	277324.988736	52.872986
3199.564270	277152.852650	52.877991
3199.181537	276984.287239	52.882996
3198.066642	276826.916404	52.888001
3197.128292	276663.226934	52.893005
3196.963035	276491.774619	52.898010
3196.178040	276340.540375	52.903015
3195.895610	276165.388196	52.908020
3195.378102	276008.483101	52.913025
3194.342186	275846.031509	52.918029
3193.967677	275665.036149	52.923034
3193.006036	275509.627541	52.928039
3192.353110	275327.606551	52.933044
3191.526981	275171.412446	52.938049
3190.820706	274999.128821	52.943053
3190.537871	274829.019417	52.948058
3189.473099	274665.044276	52.953063
3189.215182	274502.495045	52.958068
3188.464055	274344.073330	52.963073
3187.891178	274176.098238	52.968077
3187.328474	274007.815922	52.973082
3186.349655	273846.424981	52.978087
3185.575841	273674.585041	52.983092
3185.182171	273500.647491	52.988097
3184.479215	273340.384475	52.993101
3183.999723	273164.346652	52.998106
3183.105976	273018.197863	53.003111
3182.489863	272833.344157	53.008116
3181.727268	272668.455385	53.013121
3180.886705	272510.964794	53.018125
3180.527863	272342.803155	53.023130
3179.658989	272186.692368	53.028135
3178.852070	272017.888551	53.033140
3178.504729	271854.334924	53.038145
3177.554951	271689.323070	53.043149
3177.063305	271512.243155	53.048154
3176.128777	271363.783364	53.053159
3175.459947	271195.314369	53.058164
3174.848721	271043.390708	53.063169
3174.165521	270886.639474	53.068173
3173.835388	270719.059294	53.073178
3173.016360	270561.743834	53.078183
3172.677728	270393.833969	53.083188
3171.740582	270236.180699	53.088193
3170.895701	270060.175673	53.093197
3170.364984	269886.973425	53.098202
3169.768941	269738.511275	53.103207
3168.814991	269572.379849	53.108212
3168.585754	269411.762281	53.113217
3167.814595	269249.294908	53.118221
3167.035149	269089.324775	53.123226
3166.212820	268922.612373	53.128231
3165.817402	268754.584515	53.133236
3165.235824	268601.230409	53.138241
3164.286023	268440.192256	53.143245
3163.889083	268270.076370	53.148250
3163.156631	268100.599392	53.153255
3162.448281	267942.426546	53.158260
3161.586558	267783.233815	53.163265
3161.109384	267627.749577	53.168269
3160.547792	267457.991073	53.173274
3159.946628	267291.575219	53.178279
3159.151114	267115.766937	53.183284
3158.106230	266961.722541	53.188289
3157.199763	266801.798608	53.193293
3156.796058	266646.379441	53.198298
3156.100355	266487.975818	53.203303
3155.628400	266330.912123	53.208308
3155.238930	266180.355274	53.213313
3154.140839	266020.793011	53.218317
3153.918898	265851.694424	53.223322
3152.995009	265693.683737	53.228327
3152.561312	265539.695905	53.233332
3151.688145	265377.194920	53.238337
3151.028856	265217.767261	53.243341
3150.549214	265037.783961	53.248346
3149.793731	264888.864501	53.253351
3149.081064	264724.148122	53.258356
3148.584541	264562.835796	53.263361
3147.777610	264406.335180	53.268365
3147.111340	264239.905305	53.273370
3146.326577	264083.172102	53.278375
3145.958288	263923.851728	53.283380
3145.092245	263761.324818	53.288385
3144.107557	263609.360501	53.293389
3143.732787	263441.000231	53.298394
3142.623813	263286.763603	53.303399
3142.248531	263129.252916	53.308404
3141.779325	262980.696411	53.313409
3140.847460	262814.156423	53.318413
3140.249620	262652.300693	53.323418
3139.644511	262502.721722	53.328423
3139.072099	262333.170820	53.333428
3138.429293	262190.397886	53.338433
3137.517343	262035.239288	53.343437
3137.169352	261871.001371	53.348442
3136.317590	261712.726331	53.353447
3135.760480	261544.548697	53.358452
3135.133378	261388.071958	53.363457
3134.228779	261236.911049	53.368461
3133.544896	261073.388881	53.373466
3132.685517	260927.951227	53.378471
3132.576272	260771.851287	53.383476
3131.611494	260610.003769	53.388481
3131.001575	260457.090297	53.393485
3130.227982	260291.774565	53.398490
3129.414632	260145.820675	53.403495
3129.081718	259977.022723	53.408500
3128.429178	259835.245720	53.413505
3128.005261	259679.170724	53.418509
3127.356112	259519.056640	53.423514
3126.266643	259355.625140	53.428519
3126.003139	259188.599438	53.433524
3125.315596	259038.245821	53.438529
3124.411993	258881.916135	53.443533
3123.843191	258715.193733	53.448538
3122.872009	258559.384293	53.453543
3122.312446	258396.913723	53.458548
3121.845529	258240.617204	53.463553
3121.099205	258095.086820	53.468557
3120.580834	257932.482703	53.473562
3119.612700	257780.900884	53.478567
3118.853675	257618.156795	53.483572
3118.299386	257459.047729	53.488577
3117.802122	257312.281443	53.493581
3117.392179	257152.080114	53.498586
3116.193274	256996.740685	53.503591
3116.118350	256837.734461	53.508596
3115.031381	256685.764693	53.513601
3114.521049	256538.695368	53.518605
3114.031411	256364.678456	53.523610
3113.158722	256219.500337	53.528615
3112.616567	256045.823065	53.533620
3112.068762	255897.690479	53.538625
3110.892034	255741.533480	53.543629
3110.283244	255577.646552	53.548634
3109.491051	255425.631023	53.553639
3109.133527	255273.470413	53.558644
3108.408860	255116.631128	53.563649
3107.705673	254963.099292	53.568653
3107.118421	254803.080576	53.573658
3106.294799	254661.613974	53.578663
3105.812018	254502.419378	53.583668
3105.069023	254343.826367	53.588673
3104.302766	254195.958787	53.593677
3104.090985	254038.071431	53.598682
3102.926830	253888.764502	53.603687
3102.505781	253727.243270	53.608692
3101.457075	253566.534582	53.613697
3100.852619	253415.025687	53.618701
3100.586521	253257.071170	53.623706
3099.622818	253115.373200	53.628711
3099.223638	252959.095345	53.633716
3098.615741	252795.210598	53.638721
3097.791545	252645.901789	53.643725
3097.703273	252487.665117	53.648730
3096.712280	252333.900804	53.653735
3096.226187	252166.584798	53.658740
3095.547967	252014.324732	53.663745
3094.479481	251849.724269	53.668749
3093.798146	251687.736692	53.673754
3092.807716	251548.259789	53.678759
3092.548038	251395.704820	53.683764
3091.803591	251248.243633	53.688769
3090.971605	251086.917127	53.693773
3090.450031	250933.156155	53.698778
3089.966284	250784.966512	53.703783
3089.229202	250621.970102	53.708788
3088.425892	250476.327029	53.713793
3087.740505	250316.760716	53.718797
3087.369938	250158.698186	53.723802
3086.314675	250018.188686	53.728807
3085.808565	249866.183438	53.733812
3085.175681	249703.171448	53.738817
3084.352735	249556.513646	53.743821
3083.983698	249405.582193	53.748826
3083.099820	249250.657753	53.753831
3082.755529	249094.935010	53.758836
3081.746839	248946.168001	53.763841
3081.237338	248793.043799	53.768845
3080.702862	248633.124219	53.773850
3079.504371	248481.484546	53.778855
3079.014517	248322.500475	53.783860
3078.644537	248177.427578	53.788865
3077.700200	248035.578056	53.793869
3077.291123	247877.447514	53.798874
3076.041170	247715.808577	53.803879
3076.225246	247559.927370	53.808884
3075.411577	247415.027296	53.813889
3074.592001	247258.337547	53.818893
3074.172380	247097.968497	53.823898
3073.044304	246945.988179	53.828903
3072.383367	246793.526631	53.833908
3072.229591	246639.660749	53.838913
3071.420061	246487.273976	53.843917
3070.941436	246337.738096	53.848922
3069.657851	246186.292512	53.853927
3069.128436	246023.191732	53.858932
3068.700967	245869.089879	53.863937
3067.663717	245723.539324	53.868941
3067.359851	245566.998998	53.873946
3066.289319	245419.085722	53.878951
3065.683188	245263.484878	53.883956
3065.189172	245113.417968	53.888961
3064.209178	244970.431174	53.893965
3063.907957	244820.588727	53.898970
3062.882793	244675.648547	53.903975
3062.632653	244535.169645	53.908980
3062.230897	244381.752965	53.913985
3061.191351	244221.536276	53.918989
3060.575684	244062.194911	53.923994
3059.853094	243925.305657	53.928999
3059.001510	243776.417319	53.934004
3058.654927	243634.350322	53.939009
3057.789688	243477.875821	53.944013
3057.529577	243320.465377	53.949018
3056.368389	243184.945053	53.954023
3056.037880	243032.995664	53.959028
3055.233485	242883.056815	53.964033
3054.239872	242726.883669	53.969037
3053.819787	242569.855984	53.974042
3053.385698	242436.564166	53.979047
3052.438408	242290.060961	53.984052
3051.917722	242130.834291	53.989057
3051.069474	241982.635082	53.994061
3050.704715	241837.975548	53.999066
3049.906955	241688.724638	54.004071
3049.241441	241539.631232	54.009076
3048.752785	241394.126026	54.014081
3047.634322	241239.884385	54.019085
3047.057345	241086.779544	54.024090
3046.418357	240940.891243	54.029095
3045.801294	240793.217117	54.034100
3045.335151	240654.482864	54.039105
3044.602281	240507.540436	54.044109
3044.159911	240346.623048	54.049114
3043.390732	240196.249028	54.054119
3042.813800	240046.252205	54.059124
3042.002598	239897.336703	54.064129
3041.153369	239743.818334	54.069133
3040.614015	239600.385983	54.074138
3039.918345	239451.809270	54.079143
3039.303196	239293.747243	54.084148
3038.401036	239159.489131	54.089153
3037.525329	239014.073605	54.094157
3037.503035	238857.828169	54.099162
3036.584359	238721.586974	54.104167
3035.786253	238565.464745	54.109172
3035.336634	238414.329487	54.114177
3034.668100	238276.852422	54.119181
3034.186517	238122.615989	54.124186
3033.508032	237967.545159	54.129191
3032.848726	237819.244956	54.134196
3032.249024	237669.891494	54.139201
3031.630040	237520.846855	54.144205
3031.082830	237361.732792	54.149210
3029.778361	237223.084512	54.154215
3029.203701	237061.581625	54.159220
3028.801095	236917.188927	54.164225
3028.197448	236763.788586	54.169229
3027.453349	236617.056748	54.174234
3026.377433	236477.838518	54.179239
3025.921614	236332.385558	54.184244
3025.475236	236185.199773	54.189249
3024.587612	236033.475119	54.194253
3023.932520	235881.382850	54.199258
3023.146380	235731.144925	54.204263
3022.285776	235580.613442	54.209268
3021.686016	235432.689093	54.214273
3021.306522	235289.771856	54.219277
3020.630475	235131.751019	54.224282
3019.938354	234999.349145	54.229287
3019.157891	234853.745942	54.234292
3018.537061	234711.376984	54.239297
3017.826696	234571.441413	54.244301
3017.693373	234410.000097	54.249306
3016.732541	234271.250437	54.254311
3015.866838	234124.745105	54.259316
3015.123148	233969.970617	54.264321
3014.428354	233829.728061	54.269325
3013.962746	233687.870714	54.274330
3013.510696	233549.983657	54.279335
3012.504931	233399.554800	54.284340
3012.146459	233252.486672	54.289345
3010.991641	233112.368885	54.294349
3010.529110	232959.588515	54.299354
3009.989077	232824.950195	54.304359
3009.339972	232682.766875	54.309364
3009.007061	232524.008379	54.314369
3008.119699	232377.101691	54.319373
3007.440593	232232.632142	54.324378
3006.526397	232095.609657	54.329383
3006.073290	231944.917347	54.334388
3005.084355	231806.786756	54.339393
3004.255426	231659.362678	54.344397
3004.285673	231514.043522	54.349402
3003.163787	231382.580311	54.354407
3002.802374	231233.733384	54.359412
3002.293495	231080.224962	54.364417
3001.452077	230936.674282	54.369421
3000.835850	230790.618334	54.374426
3000.011716	230648.542179	54.379431
2999.554662	230500.730061	54.384436
2999.020647	230360.823638	54.389441
2998.033547	230212.459339	54.394445
2997.658888	230054.806517	54.399450
2997.119234	229921.572729	54.404455
2996.344202	229765.460590	54.409460
2995.419204	229628.596244	54.414465
2994.744159	229477.459323	54.419469
2994.373965	229334.422199	54.424474
2993.510770	229184.996041	54.429479
2992.930212	229037.740568	54.434484
2992.060679	228895.419743	54.439489
2991.176031	228754.018162	54.444493
2990.586083	228594.619675	54.449498
2989.756663	228463.801874	54.454503
2989.022042	228315.018838	54.459508
2988.478694	228179.904090	54.464513
2987.747636	228038.301120	54.469517
2987.211467	227902.370898	54.474522
2986.654202	227770.136136	54.479527
2985.975917	227619.588536	54.484532
2985.349880	227477.842552	54.489537
2984.387706	227352.827170	54.494541
2983.967746	227204.199924	54.499546
2983.717351	227069.447920	54.504551
2982.827565	226917.076370	54.509556
2982.188061	226773.144028	54.514561
2981.162257	226633.372323	54.519565
2980.885876	226494.653417	54.524570
2980.085175	226365.030942	54.529575
2979.828112	226208.983233	54.534580
2979.036728	226061.486160	54.539585
2978.072532	225924.532047	54.544589
2977.871226	225771.340679	54.549594
2977.033128	225632.444794	54.554599
2976.182782	225484.474326	54.559604
2975.457373	225338.826730	54.564609
2974.815380	225189.932684	54.569613
2974.270881	225039.075738	54.574618
2973.544614	224913.593835	54.579623
2972.641240	224773.131186	54.584628
2972.297806	224627.360736	54.589633
2971.240728	224483.587601	54.594637
2971.046276	224336.368307	54.599642
2970.207830	224194.305111	54.604647
2969.140200	224057.752414	54.609652
2968.466238	223920.284709	54.614657
2967.871554	223777.037952	54.619661
2967.061778	223641.196223	54.624666
2966.315086	223510.920505	54.629671
2965.748968	223368.382847	54.634676
2965.544089	223231.325813	54.639681
2964.727928	223103.926018	54.644685
2964.368214	222962.132948	54.649690
2963.622012	222831.769167	54.654695
2963.159651	222685.320958	54.659700
2962.057965	222540.158121	54.664705
2961.144027	222402.641950	54.669709
2960.813877	222256.275457	54.674714
2959.784794	222128.656371	54.679719
2959.203470	221988.478661	54.684724
2958.696117	221845.527133	54.689729
2957.925819	221708.384083	54.694733
2957.335724	221570.830858	54.699738
2956.599181	221446.629083	54.704743
2955.863322	221301.296103	54.709748
2955.438612	221169.458513	54.714753
2954.426397	221031.425718	54.719757
2953.944821	220886.511543	54.724762
2953.439368	220757.678918	54.729767
2952.789102	220627.787425	54.734772
2952.023594	220482.817145	54.739777
2951.199835	220354.506601	54.744781
2950.735625	220214.708250	54.749786
2950.073879	220076.481704	54.754791
2949.375380	219938.044833	54.759796
2948.835658	219812.172503	54.764801
2947.900471	219676.854120	54.769805
2947.773543	219529.786081	54.774810
2946.747374	219403.571395	54.779815
2946.222203	219256.299638	54.784820
2945.700105	219116.308864	54.789825
2944.883870	218982.945976	54.794829
2944.463209	218834.360135	54.799834
2943.383272	218696.698841	54.804839
2942.528919	218565.213956	54.809844
2942.001089	218422.628665	54.814849
2941.201298	218281.346904	54.819853
2940.940067	218143.709793	54.824858
2939.880467	218021.130619	54.829863
2939.298886	217883.379250	54.834868
2939.128932	217743.742717	54.839873
2937.935825	217608.672704	54.844877
2937.376829	217471.262242	54.849882
2936.599625	217339.767396	54.854887
2936.160159	217195.859479	54.859892
2935.581407	217071.436485	54.864897
2934.834693	216935.215123	54.869901
2934.416372	216786.913211	54.874906
2933.647078	216651.001470	54.879911
2932.453197	216512.789650	54.884916
2931.907203	216384.607678	54.889921
2931.534067	216267.090777	54.894925
2931.110108	216119.185771	54.899930
2930.425460	215988.824403	54.904935
2929.499000	215851.806251	54.909940
2928.998590	215711.729667	54.914945
2927.640324	215576.473352	54.919949
2927.334446	215445.620266	54.924954
2926.549707	215315.594240	54.929959
2926.073898	215174.687498	54.934964
2925.429851	215042.514038	54.939969
2924.691806	214916.490886	54.944973
2924.457171	214770.022600	54.949978
2923.742701	214642.201502	54.954983
2922.789812	214503.230056	54.959988
2922.320110	214364.398775	54.964993
2921.738091	214232.471648	54.969997
2921.173160	214094.126956	54.975002
2920.157694	213955.802972	54.980007
2919.184180	213831.168345	54.985012
2918.837121	213698.695935	54.990017
2917.842654	213568.146444	54.995021
2917.551509	213423.179261	55.000026
2916.721096	213306.567235	55.005031
2916.083567	213168.363248	55.010036
2915.639520	213034.660156	55.015041
2914.603490	212914.377474	55.020045
2914.348011	212771.900799	55.025050
2913.380650	212643.665374	55.030055
2912.819110	212504.012475	55.035060
2912.323139	212359.207351	55.040065
2911.237992	212235.522574	55.045069
2910.882847	212107.178541	55.050074
2910.194223	211981.764092	55.055079
2909.790018	211837.963841	55.060084
2909.088137	211706.900806	55.065089
2908.155302	211574.767278	55.070093
2907.909990	211436.377587	55.075098
2907.252823	211307.281110	55.080103
2906.322864	211172.067814	55.085108
2905.711570	211036.269778	55.090113
2905.068936	210902.755268	55.095117
2904.715588	210761.673127	55.100122
2903.721561	210630.633103	55.105127
2903.169945	210491.084830	55.110132
2902.720210	210362.313804	55.115137
2901.550819	210218.218353	55.120141
2901.047085	210072.694158	55.125146
2900.325411	209950.979952	55.130151
2899.334832	209809.746290	55.135156
2899.001675	209680.169095	55.140161
2898.235094	209551.169899	55.145165
2897.774402	209425.215314	55.150170
2897.089234	209292.169150	55.155175
2896.327504	209148.304351	55.160180
2895.639675	209019.930161	55.165185
2894.612171	208883.846325	55.170189
2894.188859	208761.552656	55.175194
2893.732655	208631.335315	55.180199
2892.875910	208505.267137	55.185204
2892.413100	208368.115024	55.190209
2891.939621	208231.435816	55.195213
2891.348640	208093.859161	55.200218
2890.529394	207961.855287	55.205223
2889.852952	207834.487226	55.210228
2889.324809	207698.403320	55.215233
2888.414695	207570.372825	55.220237
2887.977401	207415.935417	55.225242
2887.260401	207287.887668	55.230247
2886.406045	207152.620271	55.235252
2885.303304	207023.921454	55.240257
2884.630894	206893.627537	55.245261
2884.297959	206768.180017	55.250266
2883.308777	206640.724010	55.255271
2882.632876	206508.204278	55.260276
2882.282097	206379.667770	55.265281
2881.414626	206259.931232	55.270285
2881.015857	206131.288319	55.275290
2880.359938	205999.275632	55.280295
2879.527669	205862.633179	55.285300
2878.891804	205739.170268	55.290305
2878.038613	205609.760488	55.295309
2877.862796	205474.796722	55.300314
2876.942503	205359.181090	55.305319
2876.132070	205225.272888	55.310324
2875.737332	205093.691763	55.315329
2874.941345	204966.157882	55.320333
2874.284707	204834.656995	55.325338
2873.294136	204713.823176	55.330343
2872.629923	204584.398474	55.335348
2872.134469	204467.330157	55.340353
2871.220523	204343.417908	55.345357
2870.624396	204206.894661	55.350362
2870.469659	204092.114805	55.355367
2869.506729	203962.089760	55.360372
2869.318555	203823.275717	55.365377
2868.412779	203702.710572	55.370381
2867.496738	203573.226214	55.375386
2866.878713	203444.802139	55.380391
2866.468254	203323.281252	55.385396
2865.676045	203187.605965	55.390401
2864.826511	203059.703015	55.395405
2864.613278	202921.836870	55.400410
2863.646847	202802.835824	55.405415
2862.653986	202674.930990	55.410420
2862.426064	202554.935423	55.415425
2861.639310	202427.354841	55.420429
2861.038937	202297.339830	55.425434
2860.263714	202176.782718	55.430439
2859.652280	202040.941582	55.435444
2859.037151	201916.351023	55.440449
2858.356987	201793.641740	55.445453
2857.687272	201662.010283	55.450458
2856.851802	201539.873364	55.455463
2856.614998	201420.174334	55.460468
2855.614810	201288.392485	55.465473
2854.910037	201160.318248	55.470477
2854.488006	201028.152773	55.475482
2853.457402	200911.100234	55.480487
2852.956690	200783.923528	55.485492
2852.736088	200647.222206	55.490497
2851.760490	200532.210582	55.495501
2850.972873	200390.980322	55.500506
2850.379651	200265.906453	55.505511
2849.871437	200148.861897	55.510516
2849.259259	200014.858338	55.515521
2848.566589	199887.332357	55.520525
2848.039781	199758.304267	55.525530
2847.195674	199624.249325	55.530535
2846.615866	199500.218574	55.535540
2846.095106	199363.924320	55.540545
2845.031949	199246.091556	55.545549
2844.514370	199103.103981	55.550554
2843.730203	198984.336845	55.555559
2842.980979	198859.074610	55.560564
2842.720234	198733.022704	55.565569
2841.870210	198610.500191	55.570573
2840.971825	198472.142919	55.575578
2840.251853	198368.484359	55.580583
2839.639362	198233.149165	55.585588
2839.232739	198110.990234	55.590593
2837.739844	197986.025979	55.595597
2837.595005	197863.240814	55.600602
2837.011791	197740.678057	55.605607
2836.303558	197621.151176	55.610612
2836.032290	197497.890614	55.615617
2835.038095	197369.209545	55.620621
2834.651543	197241.768660	55.625626
2833.817495	197125.876664	55.630631
2833.071151	196991.952854	55.635636
2832.976414	196862.926988	55.640641
2831.539074	196753.684569	55.645645
2831.185202	196623.186103	55.650650
2830.441689	196505.079793	55.655655
2829.639285	196369.524992	55.660660
2829.064277	196251.532543	55.665665
2828.422908	196128.664669	55.670669
2827.810548	196000.130108	55.675674
2827.100044	195880.989314	55.680679
2826.282476	195756.521505	55.685684
2826.085651	195630.326969	55.690689
2824.972818	195512.090558	55.695693
2824.735072	195387.659059	55.700698
2823.910959	195266.858076	55.705703
2823.316530	195135.663467	55.710708
2822.987467	195010.916517	55.715713
2821.761882	194889.111179	55.720717
2821.270274	194759.020984	55.725722
2820.418369	194643.340993	55.730727
2819.785311	194512.344972	55.735732
2819.208142	194380.131654	55.740737
2818.200038	194273.358639	55.745741
2817.727837	194147.771249	55.750746
2817.151945	194027.442868	55.755751
2816.618813	193900.058942	55.760756
2816.035348	193776.780408	55.765761
2815.361160	193658.567923	55.770765
2814.861071	193527.566131	55.775770
2813.895908	193397.198186	55.780775
2813.314291	193278.043103	55.785780
2812.761459	193147.279690	55.790785
2811.811479	193029.697667	55.795789
2811.451827	192899.273298	55.800794
2810.749447	192780.520244	55.805799
2809.926102	192651.798593	55.810804
2809.423477	192529.693640	55.815809
2808.663578	192407.756971	55.820813
2808.383564	192281.545838	55.825818
2807.233513	192155.943594	55.830823
2806.408951	192025.964146	55.835828
2806.371785	191903.252641	55.840833
2805.408832	191778.423308	55.845837
2804.860730	191642.433821	55.850842
2804.250657	191525.679468	55.855847
2803.314008	191397.411645	55.860852
2802.704478	191275.453980	55.865857
2802.119719	191152.360330	55.870861
2801.576017	191024.158488	55.875866
2800.731292	190895.928323	55.880871
2800.011189	190777.144767	55.885876
2799.675874	190649.432561	55.890881
2798.386584	190531.643099	55.895885
2797.543457	190398.515624	55.900890
2797.395175	190293.599856	55.905895
2796.687328	190164.433902	55.910900
2796.079466	190037.491695	55.915905
2795.283829	189927.170230	55.920909
2794.880122	189791.430260	55.925914
2794.080214	189670.651867	55.930919
2793.352221	189547.572285	55.935924
2792.703499	189421.083486	55.940929
2791.697795	189304.727973	55.945933
2791.235190	189173.553832	55.950938
2790.638741	189063.240988	55.955943
2790.157759	188942.350319	55.960948
2789.449127	188823.849698	55.965953
2788.513503	188700.474413	55.970957
2788.361074	188574.888905	55.975962
2787.554172	188457.244459	55.980967
2786.740353	188331.268179	55.985972
2786.100144	188195.074065	55.990977
2785.244434	188084.906355	55.995981
2784.774973	187963.532923	56.000986
2784.227868	187848.138883	56.005991
2783.802080	187715.805239	56.010996
2782.912098	187588.583514	56.016001
2781.915025	187472.447450	56.021005
2781.959335	187337.356028	56.026010
2780.934219	187212.281346	56.031015
2780.067961	187089.293715	56.036020
2779.552322	186963.897286	56.041025
2778.799184	186847.685984	56.046029
2778.135757	186712.861147	56.051034
2777.636857	186603.518256	56.056039
2776.675669	186485.139915	56.061044
2776.046832	186352.498834	56.066049
2775.128299	186241.022378	56.071053
2774.440385	186111.966204	56.076058
2773.375314	185996.086345	56.081063
2773.118016	185892.686143	56.086068
2772.836873	185760.805898	56.091073
2771.996477	185650.158144	56.096077
2771.822390	185531.085121	56.101082
2771.202865	185410.721746	56.106087
2770.548404	185288.723133	56.111092
2769.948413	185150.063642	56.116097
2768.580882	185036.498582	56.121101
2768.074148	184907.722443	56.126106
2767.612323	184786.178089	56.131111
2766.972842	184673.503620	56.136116
2766.175028	184540.423895	56.141121
2765.442597	184426.836102	56.146125
2765.070016	184301.182632	56.151130
2764.135939	184181.393935	56.156135
2763.874828	184056.206904	56.161140
2762.925010	183928.292473	56.166145
2762.042002	183817.706851	56.171149
2762.049825	183685.850501	56.176154
2761.351560	183565.695352	56.181159
2760.443196	183443.996388	56.186164
2759.842970	183314.552695	56.191169
2759.071884	183193.735869	56.196173
2758.307221	183058.174707	56.201178
2757.707278	182949.645374	56.206183
2756.801996	182817.045771	56.211188
2756.437309	182702.055708	56.216193
2756.055548	182582.832600	56.221197
2755.536007	182447.832365	56.226202
2754.415451	182332.225192	56.231207
2753.541058	182196.137068	56.236212
2752.798375	182076.247422	56.241217
2752.221408	181962.425064	56.246221
2751.782032	181838.951672	56.251226
2750.919330	181729.080425	56.256231
2750.445132	181596.912328	56.261236
2749.867928	181467.788439	56.266241
2748.973828	181355.964143	56.271245
2748.588493	181224.635375	56.276250
2747.502991	181103.047285	56.281255
2747.176475	180975.424323	56.286260
2746.445809	180859.339526	56.291265
2745.388300	180732.367329	56.296269
2745.125399	180609.340130	56.301274
2744.270667	180491.228009	56.306279
2743.837232	180373.850850	56.311284
2743.217968	180248.298926	56.316289
2742.358079	180138.647516	56.321293
2741.651510	180004.282350	56.326298
2740.989597	179887.553279	56.331303
2740.176215	179768.291791	56.336308
2739.561770	179643.618560	56.341313
2738.884454	179533.939780	56.346317
2738.549517	179402.812109	56.351322
2738.017238	179301.658750	56.356327
2736.985311	179174.916080	56.361332
2736.509894	179045.312709	56.366337
2735.969808	178931.543400	56.371341
2735.267045	178810.282788	56.376346
2734.538573	178682.832092	56.381351
2733.619265	178554.814186	56.386356
2733.082518	178446.667753	56.391361
2732.235599	178323.116401	56.396365
2731.745280	178197.308436	56.401370
2731.133502	178082.458890	56.406375
2730.318374	177962.808460	56.411380
2729.807893	177835.580189	56.416385
2729.062621	177721.719458	56.421389
2728.688109	177600.435774	56.426394
2728.088417	177477.331088	56.431399
2727.592283	177346.566051	56.436404
2726.663403	177232.506793	56.441409
2726.288011	177106.925567	56.446413
2725.742620	176973.676533	56.451418
2724.901896	176859.629772	56.456423
2724.263746	176725.849304	56.461428
2723.527262	176594.336124	56.466433
2722.637236	176472.870294	56.471437
2721.906366	176352.931329	56.476442
2721.371276	176230.443341	56.481447
2720.697326	176114.566124	56.486452
2720.021185	175986.339529	56.491457
2719.026625	175859.015940	56.496461
2719.101798	175732.375444	56.501466
2718.299177	175618.351522	56.506471
2717.374643	175486.528267	56.511476
2717.067571	175355.294431	56.516481
2716.235129	175228.163341	56.521485
2715.550327	175099.304963	56.526490
2714.816408	174985.933293	56.531495
2714.127182	174855.639187	56.536500
2713.671321	174732.290991	56.541505
2712.864879	174610.944634	56.546509
2712.208639	174472.697490	56.551514
2711.487596	174353.640411	56.556519
2710.835284	174232.652323	56.561524
2710.152751	174104.165581	56.566529
2709.257816	173992.793538	56.571533
2708.628827	173861.564659	56.576538
2708.002436	173728.911358	56.581543
2707.259242	173619.004341	56.586548
2706.901882	173488.776536	56.591553
2706.236041	173370.769224	56.596557
2705.651431	173241.290437	56.601562
2704.738442	173114.064306	56.606567
2703.975430	172994.089492	56.611572
2703.236521	172866.442316	56.616577
2702.986972	172753.445328	56.621581
2702.266593	172620.301880	56.626586
2701.779958	172511.679923	56.631591
2700.894152	172385.316626	56.636596
2700.393304	172260.622356	56.641601
2699.575893	172141.612565	56.646605
2698.725370	172002.565370	56.651610
2697.806977	171877.963892	56.656615
2697.394622	171755.877021	56.661620
2697.038333	171639.123006	56.666625
2696.201960	171522.547135	56.671629
2695.926025	171398.773768	56.676634
2694.897131	171273.619426	56.681639
2694.453648	171146.681329	56.686644
2693.979898	171012.944671	56.691649
2693.050489	170891.298488	56.696653
2692.729412	170758.199812	56.701658
2692.020988	170637.129839	56.706663
2691.135225	170506.423298	56.711668
2690.752487	170368.337879	56.716673
2689.972323	170243.770572	56.721677
2688.952809	170118.898226	56.726682
2688.072368	169998.340743	56.731687
2687.371890	169879.064970	56.736692
2687.198066	169746.048166	56.741697
2685.960453	169637.604025	56.746701
2685.604407	169509.881689	56.751706
2685.512520	169380.604626	56.756711
2684.271233	169261.454593	56.761716
2683.868340	169128.870427	56.766721
2682.980049	169010.860617	56.771725
2682.444663	168874.050956	56.776730
2681.973448	168750.342407	56.781735
2681.478232	168629.779045	56.786740
2681.007080	168489.056606	56.791745
2679.852596	168366.958095	56.796749
2679.103924	168233.020288	56.801754
2678.659493	168108.241397	56.806759
2677.666255	167979.429776	56.811764
2677.104850	167861.397163	56.816769
2676.607517	167732.164473	56.821773
2676.129022	167587.555361	56.826778
2675.430636	167474.619415	56.831783
2674.669628	167346.879457	56.836788
2674.010389	167210.998241	56.841793
2673.189433	167090.109893	56.846797
2672.619768	166955.792191	56.851802
2672.296564	166826.013657	56.856807
2671.116256	166702.424132	56.861812
2670.580009	166567.632034	56.866817
2669.803020	166447.857781	56.871821
2669.663088	166314.313532	56.876826
2669.175230	166195.219076	56.881831
2667.997733	166059.894618	56.886836
2667.310892	165932.045998	56.891841
2666.419005	165802.119516	56.896845
2665.882377	165670.446033	56.901850
2665.336425	165541.622766	56.906855
2664.860845	165416.488992	56.911860
2664.233871	165294.482188	56.916865
2663.476935	165163.188725	56.921869
2662.963906	165022.104432	56.926874
2662.265117	164895.481945	56.931879
2661.471434	164766.611616	56.936884
2660.814452	164633.066320	56.941889
2660.080408	164514.753744	56.946893
2659.290414	164390.970203	56.951898
2658.920862	164252.510863	56.956903
2657.886886	164126.757892	56.961908
2657.689713	163993.485372	56.966913
2656.854217	163870.982292	56.971917
2656.309589	163733.951291	56.976922
2655.697138	163603.797557	56.981927
2654.576671	163473.762923	56.986932
2654.490062	163337.805169	56.991937
2653.392597	163213.044439	56.996941
2653.110945	163080.564231	57.001946
2652.496855	162950.413092	57.006951
2651.307569	162820.035692	57.011956
2650.740096	162691.963282	57.016961
2649.988615	162568.205256	57.021965
2649.447244	162431.928800	57.026970
2648.696046	162309.633772	57.031975
2648.031747	162187.910250	57.036980
2647.701678	162042.956037	57.041985
2646.729082	161932.763225	57.046989
2646.145736	161794.308981	57.051994
2645.558144	161672.320766	57.056999
2645.046588	161537.276245	57.062004
2644.490922	161405.150740	57.067009
2643.615900	161279.382475	57.072013
2643.031484	161137.561724	57.077018
2642.195534	161023.421446	57.082023
2641.469409	160897.046095	57.087028
2641.150675	160755.629751	57.092033
2640.573697	160630.757372	57.097037
2639.963336	160499.444856	57.102042
2639.211415	160361.417003	57.107047
2638.551814	160225.765223	57.112052
2637.598970	160095.156867	57.117057
2636.885570	159978.368818	57.122061
2636.657532	159834.907605	57.127066
2635.471391	159705.011474	57.132071
2635.000534	159579.808150	57.137076
2634.456634	159436.195193	57.142081
2633.780180	159316.720965	57.147085
2632.911476	159184.004958	57.152090
2632.105385	159068.594933	57.157095
2631.957027	158926.612242	57.162100
2631.490094	158782.328680	57.167105
2630.410669	158663.759594	57.172109
2629.759025	158524.273767	57.177114
2629.067131	158393.770234	57.182119
2628.301717	158268.147890	57.187124
2627.838667	158133.668062	57.192129
2627.231576	158011.288768	57.197133
2626.541374	157871.354004	57.202138
2626.011172	157739.632303	57.207143
2625.105065	157601.016827	57.212148
2625.127174	157468.318752	57.217153
2624.086912	157344.383234	57.222157
2624.092316	157200.654306	57.227162
2622.661629	157061.145253	57.232167
2621.960513	156918.991387	57.237172
2621.503030	156777.371560	57.242177
2621.023907	156646.612075	57.247181
2619.990155	156505.974544	57.252186
2619.530195	156381.276792	57.257191
2618.869637	156244.115201	57.262196
2618.025980	156094.919361	57.267201
2617.284573	155970.623643	57.272205
2616.577124	155824.331181	57.277210
2616.204733	155712.956910	57.282215
2615.583750	155576.007835	57.287220
2614.933196	155429.987713	57.292225
2613.956152	155301.244483	57.297229
2613.340104	155158.715814	57.302234
2612.799792	155023.612103	57.307239
2611.949210	154886.854731	57.312244
2611.964297	154749.770063	57.317249
2610.862750	154627.392226	57.322253
2610.342278	154471.643977	57.327258
2610.054411	154338.740227	57.332263
2608.812565	154209.064336	57.337268
2608.329596	154055.396740	57.342273
2607.885014	153926.269306	57.347277
2607.253697	153781.867597	57.352282
2606.615572	153648.411939	57.357287
2605.482747	153517.742682	57.362292
2605.105491	153368.065500	57.367297
2604.157415	153231.889600	57.372301
2603.636830	153098.913241	57.377306
2602.888634	152953.720126	57.382311
2602.003771	152818.895969	57.387316
2601.419867	152676.626956	57.392321
2600.998862	152547.526538	57.397325
2600.383400	152411.110628	57.402330
2599.772543	152271.478746	57.407335
2599.199015	152134.180294	57.412340
2598.975138	151989.569264	57.417345
2597.707342	151858.038185	57.422349
2597.411685	151703.792492	57.427354
2596.452071	151560.761634	57.432359
2595.694345	151416.924074	57.437364
2595.076146	151286.576085	57.442369
2594.220430	151155.287562	57.447373
2593.736929	151010.671130	57.452378
2592.631903	150868.759408	57.457383
2592.404905	150743.308542	57.462388
2591.778385	150597.407460	57.467393
2590.751056	150461.204713	57.472397
2590.167335	150328.770637	57.477402
2589.696220	150197.361465	57.482407
2589.296099	150062.370110	57.487412
2588.749304	149930.376647	57.492417
2588.209870	149715.197495	57.497421
2587.726875	149571.108464	57.502426
2586.759181	149425.406510	57.507431
2586.402070	149286.026763	57.512436
2585.578936	149136.159899	57.517441
2584.572376	148987.987731	57.522445
2584.044455	148839.333695	57.527450
2583.410326	148705.033260	57.532455
2582.722783	148568.987975	57.537460
2582.187018	148417.197949	57.542465
2581.613139	148277.437514	57.547469
2580.880794	148141.642613	57.552474
2579.755765	148003.915203	57.557479
2578.994958	147858.022348	57.562484
2578.648139	147708.099375	57.567489
2577.788611	147577.130994	57.572493
2577.435997	147426.600236	57.577498
2577.264329	147288.775665	57.582503
2576.384989	147139.613319	57.587508
2575.382211	147001.489609	57.592513
2574.872285	146855.701382	57.597517
2574.364662	146707.054047	57.602522
2573.767763	146581.563641	57.607527
2572.545951	146427.108665	57.612532
2572.184837	146273.827003	57.617537
2571.233243	146135.241464	57.622541
2570.663707	145995.248916	57.627546
2570.117850	145858.214239	57.632551
2569.507337	145717.060272	57.637556
2568.676267	145561.238685	57.642561
2567.958580	145426.533278	57.647565
2567.597952	145280.055153	57.652570
2566.896961	145145.742253	57.657575
2566.015549	144998.585506	57.662580
2565.598441	144842.498566	57.667585
2564.677590	144708.768822	57.672589
2564.163323	144565.876547	57.677594
2563.407770	144430.342733	57.682599
2562.467705	144291.306059	57.687604
2561.901315	144145.361463	57.692609
2561.164338	144003.625324	57.697613
2560.556797	143871.819176	57.702618
2559.701253	143738.146799	57.707623
2559.081776	143602.518793	57.712628
2558.981481	143463.073188	57.717633
2557.945607	143326.470397	57.722637
2557.706805	143181.456878	57.727642
2556.949856	143043.718327	57.732647
2556.014200	142898.079576	57.737652
2555.354639	142747.442070	57.742657
2554.870785	142623.665117	57.747661
2554.196946	142472.751672	57.752666
2553.565576	142328.261837	57.757671
2552.974883	142187.273276	57.762676
2552.493942	142048.453505	57.767681
2551.461834	141901.221042	57.772685
2550.805817	141760.282923	57.777690
2550.101449	141625.604680	57.782695
2549.423697	141476.907694	57.787700
2548.788114	141325.066295	57.792705
2548.136506	141193.126166	57.797709
2547.805981	141057.501754	57.802714
2547.259285	140911.264473	57.807719
2546.557935	140770.795550	57.812724
2546.258829	140613.250188	57.817729
2545.018718	140468.789431	57.822733
2544.318713	140319.415531	57.827738
2543.916062	140179.753311	57.832743
2543.243246	140040.541140	57.837748
2542.836804	139874.694376	57.842753
2541.774705	139741.097677	57.847757
2541.319261	139581.879931	57.852762
2540.687151	139441.126714	57.857767
2539.708208	139297.405232	57.862772
2539.173707	139150.285191	57.867777
2538.333665	139009.643192	57.872781
2537.751012	138857.221401	57.877786
2537.318237	138708.766065	57.882791
2536.016040	138577.118403	57.887796
2535.916096	138425.295688	57.892801
2535.029464	138283.902196	57.897805
2534.728214	138147.816204	57.902810
2534.237345	137984.089636	57.907815
2533.194905	137844.615961	57.912820
2533.095627	137685.529763	57.917825
2532.188930	137545.769184	57.922829
2531.565836	137390.807688	57.927834
2530.754075	137252.481779	57.932839
2530.273423	137094.589916	57.937844
2529.741050	136946.819830	57.942849
2528.854751	136793.097412	57.947853
2528.280137	136644.852773	57.952858
2527.324073	136491.041361	57.957863
2526.612576	136346.097622	57.962868
2526.175522	136189.169235	57.967873
2525.553400	136049.065773	57.972877
2524.682215	135890.022703	57.977882
2523.889511	135737.294611	57.982887
2523.491029	135594.566286	57.987892
2522.994297	135447.941466	57.992897
2522.068730	135299.327350	57.997901
2521.555294	135141.082819	58.002906
2520.872912	134990.272120	58.007911
2520.031605	134851.123824	58.012916
2519.536948	134698.874795	58.017921
2518.934776	134540.495166	58.022925
2518.124560	134394.954332	58.027930
2517.358977	134240.019446	58.032935
2516.390723	134099.179954	58.037940
2516.183085	133940.918927	58.042945
2515.374358	133811.932982	58.047949
2514.651687	133660.246402	58.052954
2514.326876	133498.601975	58.057959
2513.596706	133358.287307	58.062964
2512.714180	133209.054699	58.067969
2512.140373	133054.705544	58.072973
2511.424412	132908.534868	58.077978
2510.798650	132770.315178	58.082983
2510.097517	132614.210220	58.087988
2509.593762	132467.677901	58.092993
2508.757654	132305.752890	58.097997
2508.361807	132162.876030	58.103002
2507.685863	132023.092832	58.108007
2506.930542	131873.999480	58.113012
2506.329970	131725.822343	58.118017
2505.783764	131577.281706	58.123021
2505.327746	131424.180233	58.128026
2504.339415	131261.955059	58.133031
2503.468822	131107.269766	58.138036
2502.858786	130960.939909	58.143041
2502.200862	130807.048171	58.148045
2501.532874	130664.653874	58.153050
2501.163962	130502.919167	58.158055
2500.363628	130360.750615	58.163060
2499.785481	130216.832866	58.168065
2498.742574	130069.141002	58.173069
2498.545295	129906.518834	58.178074
2497.863702	129760.358994	58.183079
2496.927543	129616.831312	58.188084
2496.748852	129463.607657	58.193089
2495.805065	129309.744054	58.198093
2495.251364	129143.220099	58.203098
2494.726371	129003.936033	58.208103
2493.905880	128841.050534	58.213108
2493.327811	128683.296777	58.218113
2492.651469	128533.611734	58.223117
2492.087677	128383.655648	58.228122
2491.209269	128225.304373	58.233127
2490.636067	128071.465101	58.238132
2490.202545	127908.790458	58.243137
2489.316040	127759.600136	58.248141
2488.691949	127613.404391	58.253146
2487.720666	127450.601791	58.258151
2487.326736	127306.822330	58.263156
2486.853389	127140.043700	58.268161
2485.753252	126998.498707	58.273165
2485.144415	126839.236378	58.278170
2484.511480	126683.318854	58.283175
2483.924310	126540.056640	58.288180
2483.460497	126371.998498	58.293185
2482.892377	126221.788198	58.298189
2482.025335	126065.098537	58.303194
2481.433468	125905.191287	58.308199
2480.462088	125766.413462	58.313204
2480.142349	125603.518584	58.318209
2479.328865	125453.960986	58.323213
2478.742574	125287.503665	58.328218
2478.417242	125139.978485	58.333223
2477.082174	124972.740155	58.338228
2476.639657	124822.530385	58.343233
2476.289094	124676.319728	58.348237
2475.142855	124529.677243	58.353242
2474.743587	124369.024699	58.358247
2473.961397	124217.170511	58.363252
2473.618476	124059.393485	58.368257
2472.373285	123911.893850	58.373261
2472.073761	123747.825995	58.378266
2471.523026	123598.275135	58.383271
2470.295701	123437.505457	58.388276
2469.867918	123280.660743	58.393281
2469.226113	123128.930146	58.398285
2468.978473	122975.131627	58.403290
2468.002449	122825.398545	58.408295
2467.374250	122671.217675	58.413300
2466.929215	122512.996130	58.418305
2466.235300	122363.271720	58.423309
2465.640612	122205.266197	58.428314
2465.184293	122044.128753	58.433319
2463.956822	121897.450107	58.438324
2463.523008	121736.641103	58.443329
2462.890743	121576.143878	58.448333
2462.407605	121431.254439	58.453338
2461.830496	121267.296664	58.458343
2460.938259	121113.357172	58.463348
2460.508494	120948.311457	58.468353
2459.506829	120790.607455	58.473357
2459.024220	120635.551966	58.478362
2458.586020	120476.414646	58.483367
2457.599504	120319.561764	58.488372
2457.081370	120168.285626	58.493377
2456.156685	120009.126690	58.498381
2455.740860	119846.142557	58.503386
2455.119750	119695.094973	58.508391
2454.477590	119530.891731	58.513396
2453.793408	119372.796789	58.518401
2452.699151	119215.307407	58.523405
2452.236240	119052.354743	58.528410
2451.776144	118900.784739	58.533415
2450.741165	118744.863132	58.538420
2450.385321	118584.892697	58.543425
2449.912545	118434.400238	58.548429
2449.184598	118269.450463	58.553434
2448.572881	118103.600961	58.558439
2447.604539	117944.994806	58.563444
2447.642084	117787.798070	58.568449
2446.615421	117625.591229	58.573453
2445.718362	117463.498167	58.578458
2445.226961	117306.845253	58.583463
2444.211755	117157.969672	58.588468
2443.643627	116993.694620	58.593473
2443.136776	116846.073255	58.598477
2442.222350	116680.928362	58.603482
2441.855655	116527.434198	58.608487
2441.358091	116373.263482	58.613492
2440.545329	116205.515783	58.618497
2439.591249	116051.057584	58.623501
2439.221783	115887.386531	58.628506
2438.585723	115728.474826	58.633511
2437.433162	115561.940440	58.638516
2437.351419	115412.184423	58.643521
2436.096239	115260.381115	58.648525
2436.101468	115103.980336	58.653530
2435.382328	114952.728602	58.658535
2434.352301	114786.402031	58.663540
2434.101080	114621.907965	58.668545
2433.516761	114463.478357	58.673549
2432.641729	114307.583828	58.678554
2431.791744	114135.019361	58.683559
2431.040349	113985.758761	58.688564
2430.508694	113823.884832	58.693569
2429.824735	113673.187364	58.698573
2429.119030	113503.517524	58.703578
2428.566227	113351.804756	58.708583
2427.744711	113198.713857	58.713588
2427.632621	113029.270448	58.718593
2426.672633	112885.177525	58.723597
2426.024786	112714.209159	58.728602
2425.288347	112553.607127	58.733607
2424.886739	112398.055589	58.738612
2424.154628	112227.154692	58.743617
2423.106688	112076.860910	58.748621
2422.915457	111907.228235	58.753626
2421.971808	111745.947131	58.758631
2420.658910	111596.142506	58.763636
2420.460007	111423.753734	58.768641
2419.644894	111288.576198	58.773645
2419.012522	111119.247312	58.778650
2418.379317	110973.704828	58.783655
2417.681902	110822.239829	58.788660
2417.211161	110662.007720	58.793665
2416.494806	110522.985732	58.798669
2415.779389	110356.277095	58.803674
2415.109976	110202.444436	58.808679
2414.761994	110044.519477	58.813684
2414.354580	109872.180947	58.818689
2413.595933	109730.333575	58.823693
2412.937174	109563.507112	58.828698
2411.968266	109404.967648	58.833703
2411.141958	109252.441306	58.838708
2410.687912	109090.103711	58.843713
2409.932451	108927.827674	58.848717
2409.524851	108772.065172	58.853722
2408.819379	108614.751832	58.858727
2408.064676	108452.599404	58.863732
2407.659988	108286.179225	58.868737
2406.692782	108132.635244	58.873741
2406.604454	107964.149292	58.878746
2405.817906	107802.107781	58.883751
2405.221737	107639.973718	58.888756
2404.733466	107467.607902	58.893761
2403.684323	107306.271244	58.898765
2402.964629	107131.159007	58.903770
2402.407248	106976.580243	58.908775
2401.826446	106821.841213	58.913780
2401.111260	106644.295317	58.918785
2400.341620	106491.720256	58.923789
2399.601663	106315.443354	58.928794
2399.208114	106155.342889	58.933799
2398.253761	105991.189263	58.938804
2397.709605	105828.494462	58.943809
2396.877224	105671.569386	58.948813
2396.338755	105505.272092	58.953818
2396.151493	105337.854376	58.958823
2395.109012	105179.677886	58.963828
2394.631865	105001.789195	58.968833
2393.682300	104830.441756	58.973837
2392.977621	104673.959798	58.978842
2392.191335	104512.917502	58.983847
2391.510079	104355.983472	58.988852
2391.227236	104183.925928	58.993857
2390.597153	104028.895584	58.998861
2389.691746	103871.372221	59.003866
2389.146567	103703.413718	59.008871
2388.183775	103543.421067	59.013876
2387.774953	103375.259296	59.018881
2386.818949	103208.752462	59.023885
2386.505743	103063.333847	59.028890
2385.975244	102899.426213	59.033895
2385.254898	102734.236633	59.038900
2384.635190	102566.665993	59.043905
2383.806186	102396.642956	59.048909
2383.400656	102233.525819	59.053914
2382.699284	102068.382324	59.058919
2381.598465	101904.350039	59.063924
2381.332519	101731.127804	59.068929
2380.569478	101580.645010	59.073933
2379.864031	101409.194934	59.078938
2378.994091	101255.597470	59.083943
2378.275018	101091.675301	59.088948
2378.083771	100922.855934	59.093953
2377.105789	100765.383976	59.098957
2376.401431	100596.071094	59.103962
2375.744705	100429.010105	59.108967
2375.105626	100271.487762	59.113972
2374.747393	100106.176910	59.118977
2373.541490	99950.148477	59.123981
2372.994788	99773.369745	59.128986
2372.499126	99620.567397	59.133991
2371.639990	99458.816600	59.138996
2371.601086	99298.700228	59.144001
2370.886920	99137.423452	59.149005
2370.110467	98964.848312	59.154010
2369.280190	98802.545720	59.159015
2368.524518	98637.270358	59.164020
2367.899024	98476.738953	59.169025
2366.954572	98321.124104	59.174029
2366.570748	98151.486585	59.179034
2365.922630	97992.110185	59.184039
2365.194886	97828.326749	59.189044
2364.631584	97649.879865	59.194049
2364.209578	97503.092648	59.199053
2363.206251	97329.804712	59.204058
2362.840810	97169.228571	59.209063
2361.866592	97010.005879	59.214068
2361.603202	96843.631637	59.219073
2360.579118	96676.193232	59.224077
2359.995446	96511.140662	59.229082
2359.816445	96334.463372	59.234087
2358.778421	96175.041026	59.239092
2358.056671	96007.248863	59.244097
2357.263441	95840.223980	59.249101
2356.683321	95677.320531	59.254106
2356.311279	95511.778732	59.259111
2355.402677	95355.138444	59.264116
2354.985278	95192.675652	59.269121
2354.447814	95012.679003	59.274125
2353.821060	94846.053651	59.279130
2353.143953	94674.446609	59.284135
2352.046417	94508.374043	59.289140
2351.601526	94345.071961	59.294145
2350.773152	94179.472822	59.299149
2350.157127	94016.631499	59.304154
2349.414585	93842.916803	59.309159
2348.797353	93687.541962	59.314164
2348.294759	93512.282535	59.319169
2347.776651	93347.401331	59.324173
2347.182471	93179.622770	59.329178
2346.194504	93002.675107	59.334183
2345.216431	92841.383626	59.339188
2345.138206	92667.116196	59.344193
2343.834289	92514.394888	59.349197
2343.396133	92347.193937	59.354202
2342.930607	92182.706186	59.359207
2342.408486	92011.443835	59.364212
2341.824572	91847.535352	59.369217
2340.947018	91684.042419	59.374221
2340.128447	91511.214043	59.379226
2339.777547	91350.620239	59.384231
2339.116149	91185.353024	59.389236
2338.736976	91005.712440	59.394241
2337.721046	90842.488644	59.399245
2337.093132	90666.517098	59.404250
2336.333561	90500.611187	59.409255
2335.741653	90331.363889	59.414260
2335.065832	90158.605945	59.419265
2334.525062	89995.655490	59.424269
2333.657775	89814.193628	59.429274
2333.021790	89658.615533	59.434279
2332.256238	89490.562549	59.439284
2331.519610	89316.825496	59.444289
2331.034181	89151.945160	59.449293
2330.658314	88979.846395	59.454298
2330.157491	88816.416576	59.459303
2329.348571	88650.342362	59.464308
2328.894741	88465.104626	59.469313
2327.487166	88302.190191	59.474317
2327.151683	88138.935793	59.479322
2326.361049	87953.939695	59.484327
2325.646335	87806.445187	59.489332
2325.123270	87626.119872	59.494337
2324.576667	87460.209726	59.499341
2323.776296	87295.621692	59.504346
2323.187985	87129.156489	59.509351
2322.377061	86953.694141	59.514356
2322.099745	86796.723083	59.519361
2321.032485	86631.491461	59.524365
2320.413962	86446.442984	59.529370
2320.064396	86283.312650	59.534375
2319.259469	86115.051275	59.539380
2318.665515	85939.049345	59.544385
2317.969985	85776.941287	59.549389
2316.981120	85601.746439	59.554394
2316.532508	85438.067744	59.559399
2316.022703	85264.599973	59.564404
2315.334004	85088.417236	59.569409
2314.510792	84935.413146	59.574413
2313.764087	84760.877749	59.579418
2313.349886	84584.459153	59.584423
2312.418337	84438.740041	59.589428
2311.892108	84258.938028	59.594433
2311.288435	84085.849732	59.599437
2310.685703	83913.840257	59.604442
2309.867569	83756.318142	59.609447
2309.147680	83598.078052	59.614452
2308.928510	83411.820018	59.619457
2308.052421	83237.127552	59.624461
2307.359250	83072.174854	59.629466
2306.783924	82905.550473	59.634471
2306.308506	82733.181831	59.639476
2305.578424	82561.672612	59.644481
2304.968813	82390.760483	59.649485
2304.010443	82209.536012	59.654490
2303.645534	82047.245648	59.659495
2302.638555	81873.440915	59.664500
2302.194458	81688.019736	59.669505
2301.431058	81530.784494	59.674509
2300.714755	81355.321822	59.679514
2299.997535	81181.255072	59.684519
2299.149081	81017.921273	59.689524
2298.562454	80847.239941	59.694529
2298.091522	80686.257172	59.699533
2297.596266	80509.011063	59.704538
2297.002020	80343.012175	59.709543
2296.074379	80176.579508	59.714548
2295.623261	79993.715839	59.719553
2295.143531	79829.211197	59.724557
2294.332715	79658.277344	59.729562
2293.709036	79475.033701	59.734567
2293.143312	79300.850967	59.739572
2292.326488	79131.544739	59.744577
2291.784081	78957.665385	59.749581
2290.849852	78785.655685	59.754586
2290.437232	78616.365629	59.759591
2289.572949	78439.633041	59.764596
2289.205938	78251.239365	59.769601
2288.211803	78098.166725	59.774605
2287.423220	77915.495410	59.779610
2287.099915	77737.757906	59.784615
2286.437380	77573.458698	59.789620
2285.765102	77393.935568	59.794625
2285.003763	77220.004275	59.799629
2284.322570	77055.876938	59.804634
2283.693039	76879.716214	59.809639
2282.707148	76725.473977	59.814644
2282.371133	76534.524971	59.819649
2281.495131	76369.394908	59.824653
2280.903039	76188.399668	59.829658
2280.577987	76027.715382	59.834663
2279.649398	75844.806033	59.839668
2279.012081	75680.486420	59.844673
2278.387463	75493.806438	59.849677
2277.384674	75323.997366	59.854682
2277.023279	75149.038302	59.859687
2275.915247	74994.366090	59.864692
2275.764250	74813.053415	59.869697
2275.134918	74642.918402	59.874701
2274.274068	74465.541873	59.879706
2273.676828	74291.159851	59.884711
2272.940984	74129.966598	59.889716
2272.303132	73957.146125	59.894721
2271.620011	73786.063896	59.899725
2271.206169	73620.623262	59.904730
2270.649925	73448.510126	59.909735
2269.585651	73265.747080	59.914740
2269.090985	73103.440494	59.919745
2268.321034	72929.617195	59.924750
2267.743979	72754.694179	59.929754
2267.029619	72586.002835	59.934759
2266.117783	72414.746886	59.939764
2265.997819	72238.305183	59.944769
2264.913135	72074.662515	59.949774
2264.685415	71894.047251	59.954778
2264.151893	71724.422309	59.959783
2263.491638	71546.267026	59.964788
2262.631621	71368.392079	59.969793
2262.079512	71195.081496	59.974798
2261.056130	71032.330886	59.979802
2260.654928	70842.808301	59.984807
2260.115214	70676.975011	59.989812
2259.251913	70501.616825	59.994817
2258.592908	70324.112124	59.999822
2257.886663	70157.587498	60.004826
2257.143805	69973.448255	60.009831
2256.269580	69798.433775	60.014836
2255.683503	69619.790040	60.019841
2254.910606	69456.822690	60.024846
2254.601296	69289.292350	60.029850
2254.175061	69111.501980	60.034855
2253.094452	68941.234007	60.039860
2252.929326	68758.914689	60.044865
2251.745276	68594.835297	60.049870
2251.138170	68419.980771	60.054874
2250.894524	68257.306815	60.059879
2249.688644	68078.857788	60.064884
2249.323253	67895.121565	60.069889
2248.658338	67721.042501	60.074894
2247.686547	67557.774194	60.079898
2247.245498	67378.735263	60.084903
2246.481013	67217.482618	60.089908
2246.178623	67042.009466	60.094913
2245.339411	66866.553384	60.099918
2244.575347	66695.311192	60.104922
2243.964458	66504.388256	60.109927
2243.454952	66349.764815	60.114932
2242.924339	66159.659012	60.119937
2241.922074	65993.913522	60.124942
2241.572224	65813.538345	60.129946
2240.859900	65641.404353	60.134951
2240.046133	65467.435657	60.139956
2239.602915	65292.361695	60.144961
2238.823714	65122.253589	60.149966
2238.183857	64942.166885	60.154970
2237.583047	64761.641899	60.159975
2236.576293	64597.150336	60.164980
2235.918352	64416.374866	60.169985
2235.450111	64248.634669	60.174990
2234.898077	64061.066963	60.179994
2234.337652	63884.343221	60.184999
2233.537797	63722.476406	60.190004
2232.803825	63530.130312	60.195009
2232.287382	63364.238676	60.200014
2231.514068	63193.412269	60.205018
2231.112220	63017.551556	60.210023
2229.964651	62835.396550	60.215028
2229.337489	62656.769887	60.220033
2228.584201	62492.484222	60.225038
2228.108717	62319.532109	60.230042
2227.424606	62146.009992	60.235047
2226.694874	61972.911423	60.240052
2226.430404	61797.549919	60.245057
2225.716540	61617.908430	60.250062
2224.584281	61453.862845	60.255066
2224.398101	61257.324808	60.260071
2223.577734	61094.793554	60.265076
2223.370836	60905.917021	60.270081
2222.462965	60739.822392	60.275086
2221.567670	60562.179247	60.280090
2221.061888	60380.845126	60.285095
2220.183350	60211.556489	60.290100
2219.710394	60025.466003	60.295105
2218.902787	59860.518647	60.300110
2218.555934	59672.613686	60.305114
2217.721258	59504.350076	60.310119
2216.946609	59321.340555	60.315124
2216.439537	59140.123104	60.320129
2215.844563	58976.555221	60.325134
2215.085203	58790.386348	60.330138
2214.566867	58623.128204	60.335143
2213.763176	58440.438961	60.340148
2213.023728	58248.480019	60.345153
2212.405371	58079.777151	60.350158
2211.674867	57904.256954	60.355162
2211.291315	57722.036701	60.360167
2210.521574	57543.528807	60.365172
2209.842247	57371.050321	60.370177
2209.290547	57192.558697	60.375182
2208.445892	57015.166036	60.380186
2208.115979	56836.003348	60.385191
2206.955104	56658.756056	60.390196
2206.715704	56479.224837	60.395201
2206.018279	56304.853925	60.400206
2205.230461	56128.188690	60.405210
2204.360219	55947.148676	60.410215
2203.752818	55762.546383	60.415220
2203.228553	55585.626185	60.420225
2202.644974	55418.021286	60.425230
2202.064869	55232.043357	60.430234
2201.619051	55043.685202	60.435239
2200.573027	54866.126853	60.440244
2200.061929	54683.643587	60.445249
2199.081536	54506.578320	60.450254
2198.492040	54325.493968	60.455258
2198.137170	54150.478454	60.460263
2197.009742	53977.039655	60.465268
2196.611868	53794.129615	60.470273
2195.787961	53626.664709	60.475278
2195.380190	53446.895628	60.480282
2194.361296	53263.912233	60.485287
2193.856406	53090.803983	60.490292
2193.449111	52909.075127	60.495297
2192.642110	52730.395364	60.500302
2191.845397	52563.609933	60.505306
2191.357844	52380.487880	60.510311
2190.342751	52199.919393	60.515316
2190.038520	52011.915051	60.520321
2189.102182	51843.165037	60.525326
2188.974465	51669.953589	60.530330
2188.656628	51479.470018	60.535335
2187.288106	51306.822764	60.540340
2186.739991	51106.226485	60.545345
2186.315349	50934.594231	60.550350
2185.577741	50750.756407	60.555354
2184.951710	50568.952936	60.560359
2183.693122	50400.884529	60.565364
2183.470885	50207.314556	60.570369
2182.601641	50025.030001	60.575374
2181.926359	49858.560427	60.580378
2181.245545	49682.371266	60.585383
2180.779485	49507.348800	60.590388
2180.158622	49318.382045	60.595393
2179.386360	49142.162107	60.600398
2178.423933	48963.130042	60.605402
2178.291679	48784.338206	60.610407
2177.503787	48614.339143	60.615412
2176.992169	48427.205669	60.620417
2176.092785	48250.707874	60.625422
2175.414421	48072.114234	60.630426
2174.964988	47880.057574	60.635431
2174.053369	47723.996001	60.640436
2173.579232	47535.040747	60.645441
2172.878650	47353.924066	60.650446
2172.001639	47165.432087	60.655450
2171.603608	46989.787829	60.660455
2170.784273	46815.063053	60.665460
2170.205312	46640.115249	60.670465
2169.283378	46459.786202	60.675470
2168.782093	46277.038936	60.680474
2168.480957	46095.697837	60.685479
2167.516778	45924.462093	60.690484
2166.654895	45739.958886	60.695489
2166.403445	45553.266899	60.700494
2165.485208	45382.370757	60.705498
2164.817193	45205.680130	60.710503
2163.957734	45022.531482	60.715508
2163.416424	44842.411702	60.720513
2162.606658	44684.494881	60.725518
2161.931964	44493.605251	60.730522
2161.623400	44323.555748	60.735527
2160.709773	44146.981213	60.740532
2160.153804	43968.498404	60.745537
2159.454382	43798.870250	60.750542
2159.059501	43609.169854	60.755546
2158.489654	43439.866205	60.760551
2157.468398	43253.491726	60.765556
2157.243918	43063.435025	60.770561
2156.551008	42888.963454	60.775566
2155.625130	42706.048955	60.780570
2155.133096	42531.862193	60.785575
2154.137250	42355.100727	60.790580
2153.771729	42167.767409	60.795585
2152.978769	41989.491198	60.800590
2152.212050	41805.795700	60.805594
2151.475031	41636.409728	60.810599
2151.035703	41460.422937	60.815604
2150.590621	41267.565512	60.820609
2149.634667	41103.456074	60.825614
2148.732368	40911.743985	60.830618
2148.077136	40731.454178	60.835623
2147.544826	40556.553849	60.840628
2147.091774	40374.547187	60.845633
2146.620696	40204.877011	60.850638
2145.736353	40017.208336	60.855642
2145.068094	39827.349436	60.860647
2144.562369	39667.120473	60.865652
2143.708406	39477.762879	60.870657
2142.804060	39294.846492	60.875662
2141.872471	39128.251142	60.880666
2141.711890	38942.559894	60.885671
2140.871946	38775.063428	60.890676
2140.559273	38590.751779	60.895681
2140.156383	38413.933724	60.900686
2139.380644	38229.067139	60.905690
2138.355811	38050.255405	60.910695
2138.006595	37878.258975	60.915700
2137.575253	37689.641461	60.920705
2136.814180	37505.052335	60.925710
2136.168284	37321.343216	60.930714
2135.642350	37127.516376	60.935719
2134.746762	36943.915787	60.940724
2134.003202	36750.922883	60.945729
2133.186396	36579.042310	60.950734
2132.628596	36384.214287	60.955738
2132.250200	36200.917500	60.960743
2131.207424	36030.047303	60.965748
2130.958034	35839.151860	60.970753
2130.039675	35658.907083	60.975758
2129.259128	35482.686996	60.980762
2128.809664	35296.624846	60.985767
2127.837683	35115.896548	60.990772
2127.225936	34926.714295	60.995777
2126.413056	34755.828510	61.000782
2125.820775	34581.475126	61.005786
2125.504814	34394.113749	61.010791
2124.343032	34215.803868	61.015796
2123.891072	34027.316057	61.020801
2123.367236	33853.501498	61.025806
2122.889856	33666.091730	61.030810
2121.924059	33485.435421	61.035815
2121.550865	33304.931998	61.040820
2120.637346	33122.468171	61.045825
2119.918131	32946.408946	61.050830
2119.370792	32767.048377	61.055834
2118.722855	32585.349524	61.060839
2117.813698	32416.282429	61.065844
2117.477802	32217.357565	61.070849
2117.051147	32036.757911	61.075854
2116.074507	31868.241241	61.080858
2115.790201	31661.677753	61.085863
2114.717194	31493.165983	61.090868
2114.274078	31299.460036	61.095873
2113.486041	31116.044028	61.100878
2112.709626	30926.260360	61.105882
2112.063904	30754.373275	61.110887
2111.003969	30581.085818	61.115892
2110.580434	30392.682291	61.120897
2109.911326	30216.936550	61.125902
2109.048890	30039.591199	61.130906
2108.681939	29853.450647	61.135911
2107.832383	29679.693774	61.140916
2107.498785	29496.689852	61.145921
2106.653213	29320.029013	61.150926
2105.678558	29146.773223	61.155930
2105.042608	28963.889603	61.160935
2104.090720	28788.605382	61.165940
2103.675409	28613.372193	61.170945
2103.207871	28440.523726	61.175950
2102.431817	28268.402229	61.180954
2101.831764	28094.804332	61.185959
2101.283816	27917.139875	61.190964
2100.779140	27738.806977	61.195969
2100.155077	27554.806166	61.200974
2099.315511	27390.972657	61.205978
2098.670658	27199.800693	61.210983
2097.795315	27030.292560	61.215988
2097.285467	26854.831902	61.220993
2096.657835	26681.886187	61.225998
2095.683292	26511.090456	61.231002
2095.274618	26323.983546	61.236007
2094.465032	26152.218428	61.241012
2093.977331	25975.047524	61.246017
2093.235596	25799.070419	61.251022
2092.597009	25624.043216	61.256026
2091.929471	25446.093967	61.261031
2091.170793	25272.101373	61.266036
2090.675876	25102.144831	61.271041
2089.806943	24923.647316	61.276046
2089.294624	24742.010411	61.281050
2088.729979	24578.517261	61.286055
2087.894976	24405.407797	61.291060
2087.149183	24226.910350	61.296065
2087.034417	24060.586254	61.301070
2086.045292	23881.445799	61.306074
2085.403770	23701.573838	61.311079
2084.913841	23530.966674	61.316084
2084.331419	23352.645760	61.321089
2083.671285	23169.174675	61.326094
2082.644297	23000.657879	61.331098
2082.115522	22810.322068	61.336103
2081.352480	22637.433580	61.341108
2081.008123	22451.540650	61.346113
2080.211210	22280.700278	61.351118
2079.331208	22112.239071	61.356122
2078.856171	21929.094839	61.361127
2078.182893	21762.471989	61.366132
2077.213244	21577.024911	61.371137
2076.557849	21405.779087	61.376142
2076.144490	21237.126807	61.381146
2075.386017	21063.619155	61.386151
2074.583328	20893.483974	61.391156
2074.080780	20714.628142	61.396161
2073.111556	20541.692627	61.401166
2072.531128	20374.175923	61.406170
2072.379004	20197.749105	61.411175
2071.273715	20025.140486	61.416180
2070.413112	19852.972588	61.421185
2069.917852	19683.691478	61.426190
2069.280125	19511.322213	61.431194
2068.682805	19342.610072	61.436199
2067.754386	19179.032193	61.441204
2067.045520	18997.821123	61.446209
2066.508708	18840.996966	61.451214
2065.413195	18677.365981	61.456218
2065.411646	18512.348934	61.461223
2064.344722	18341.596528	61.466228
2063.405988	18166.881269	61.471233
2063.079755	18001.660238	61.476238
2062.517889	17834.174848	61.481242
2061.888631	17670.250319	61.486247
2060.888197	17512.329774	61.491252
2060.560246	17347.231206	61.496257
2059.752672	17174.683392	61.501262
2059.250232	17015.738055	61.506266
2058.788101	16836.888944	61.511271
2057.916814	16676.069517	61.516276
2057.089340	16510.625563	61.521281
2056.433687	16346.199215	61.526286
2055.257807	16187.225586	61.531290
2055.033442	16031.119561	61.536295
2053.933678	15869.732455	61.541300
2053.058149	15704.169581	61.546305
2052.673846	15550.897194	61.551310
2051.447907	15413.565579	61.556314
2050.814927	15264.734104	61.561319
2049.966723	15120.175533	61.566324
2049.134030	14977.074617	61.571329
2048.158357	14839.186111	61.576334
2047.056428	14701.759577	61.581338
2046.650275	14572.271975	61.586343
2045.707296	14459.096125	61.591348
2044.646076	14333.616397	61.596353
2043.758996	14213.103987	61.601358
2042.957778	14105.950958	61.606362
2042.388759	13988.755589	61.611367
2041.307049	13883.763331	61.616372
2040.492125	13778.066423	61.621377
2039.816979	13675.754636	61.626382
2038.625305	13576.506790	61.631386
2037.903241	13478.568998	61.636391
2037.050735	13392.430711	61.641396
2036.885312	13298.632697	61.646401
2035.965386	13207.392937	61.651406
2034.915101	13135.319516	61.656410
2034.419747	13037.530473	61.661415
2033.406325	12959.513363	61.666420
2033.052928	12879.882438	61.671425
2032.343585	12799.512263	61.676430
2031.488165	12720.966042	61.681434
2031.104453	12636.140311	61.686439
2030.244055	12558.288588	61.691444
2029.504661	12480.447454	61.696449
2029.149637	12399.556873	61.701454
2028.590593	12329.710412	61.706458
2027.741648	12234.533204	61.711463
2026.937981	12167.418608	61.716468
2026.692591	12087.550767	61.721473
2025.811547	12009.848946	61.726478
2024.954899	11937.595406	61.731482
2024.447006	11856.999282	61.736487
2023.563886	11788.703082	61.741492
2022.892080	11712.651937	61.746497
2022.704547	11638.670646	61.751502
2021.610774	11557.202660	61.756506
2021.450998	11483.571231	61.761511
2020.739234	11413.830353	61.766516
2020.205938	11341.820093	61.771521
2019.502805	11260.882916	61.776526
2018.525452	11188.881329	61.781530
2018.161947	11107.797363	61.786535
2017.189959	11032.671559	61.791540
2016.697800	10960.708661	61.796545
2016.147182	10881.922172	61.801550
2015.512431	10807.778015	61.806554
2015.083876	10732.363087	61.811559
2013.985351	10661.935888	61.816564
2013.403207	10583.546928	61.821569
2013.183305	10516.860261	61.826574
2012.277799	10439.577128	61.831578
2011.844100	10357.633485	61.836583
2010.984139	10283.685845	61.841588
2010.133182	10205.458289	61.846593
2009.621602	10129.919494	61.851598
2008.940973	10056.127953	61.856602
2008.593453	9985.164173	61.861607
2007.785946	9907.217678	61.866612
2007.020913	9828.521213	61.871617
2006.458707	9747.407835	61.876622
2005.748009	9686.157646	61.881626
2005.411552	9600.315517	61.886631
2004.130783	9540.538316	61.891636
2003.550118	9451.874939	61.896641
2002.864410	9390.816470	61.901646
2002.380510	9312.663896	61.906650
2001.605699	9243.221958	61.911655
2000.845421	9176.706277	61.916660
2000.322647	9106.342511	61.921665
1999.600529	9036.260813	61.926670
1998.613385	8963.116187	61.931674
1997.906099	8889.280953	61.936679
1997.225556	8832.290185	61.941684
1996.437281	8763.968174	61.946689
1995.861593	8697.745235	61.951694
1995.079571	8636.795062	61.956698
1994.717399	8566.272638	61.961703
1993.638256	8524.723805	61.966708
1993.216354	8451.191377	61.971713
1992.826541	8395.127690	61.976718
1992.156668	8319.517007	61.981722
1991.507232	8262.196464	61.986727
1990.842833	8190.148709	61.991732
1990.274105	8127.134121	61.996737
1989.477377	8064.828137	62.001742
1988.762118	7999.410670	62.006746
1988.571588	7930.685966	62.011751
1987.466145	7877.319089	62.016756
1986.923542	7800.926780	62.021761
1985.687355	7732.477042	62.026766
1985.195994	7684.434630	62.031770
1984.924882	7617.497574	62.036775
1984.332942	7564.757147	62.041780
1983.612003	7510.484084	62.046785
1982.827888	7446.585935	62.051790
1982.138048	7381.360416	62.056794
1981.718412	7307.574896	62.061799
1980.720024	7252.298409	62.066804
1980.528411	7188.353862	62.071809
1979.965644	7124.481124	62.076814
1979.027883	7063.390912	62.081818
1978.556116	6995.675186	62.086823
1977.678922	6930.725133	62.091828
1977.138095	6873.526001	62.096833
1975.949687	6798.275512	62.101838
1975.315072	6740.442564	62.106842
1975.042132	6679.428650	62.111847
1974.189009	6621.679756	62.116852
1973.640845	6556.295739	62.121857
1972.722141	6510.033549	62.126862
1972.088435	6441.498064	62.131866
1971.331888	6387.050168	62.136871
1970.980894	6323.387055	62.141876
1970.381889	6268.984789	62.146881
1969.436273	6209.927765	62.151886
1968.796493	6149.373393	62.156890
1968.304351	6088.278379	62.161895
1967.101938	6039.357892	62.166900
1966.721028	5977.408762	62.171905
1966.158015	5922.105983	62.176910
1965.271489	5862.075483	62.181914
1965.151448	5811.272263	62.186919
1964.293045	5756.636189	62.191924
1963.573753	5688.194282	62.196929
1962.896183	5639.442638	62.201934
1961.699141	5576.225444	62.206938
1961.581378	5515.121479	62.211943
1960.342730	5474.448916	62.216948
1960.158164	5419.825438	62.221953
1959.447058	5359.583771	62.226958
1958.935876	5311.810892	62.231962
1958.083877	5254.389755	62.236967
1957.532338	5202.951966	62.241972
1957.100041	5144.738977	62.246977
1956.252127	5090.494922	62.251982
1955.495922	5025.698075	62.256986
1955.445413	4973.644414	62.261991
1954.435641	4920.963936	62.266996
1953.687978	4858.199840	62.272001
1953.054549	4801.230843	62.277006
1952.101045	4739.358859	62.282010
1951.637465	4691.802851	62.287015
1950.805354	4636.105912	62.292020
1950.752339	4580.374632	62.297025
1949.785650	4529.158894	62.302030
1949.078561	4467.905148	62.307034
1948.625308	4407.210783	62.312039
1947.721466	4354.901985	62.317044
1947.001944	4303.777933	62.322049
1947.045930	4236.318679	62.327054
1946.053514	4179.875984	62.332058
1945.018036	4124.500351	62.337063
1944.263730	4069.390249	62.342068
1943.758029	4002.811174	62.347073
1943.224013	3958.569386	62.352078
1942.496459	3902.827865	62.357082
1941.986426	3832.228741	62.362087
1941.093499	3792.742608	62.367092
1940.016808	3741.289971	62.372097
1939.510427	3688.853411	62.377102
1938.990471	3636.423136	62.382106
1938.653255	3586.302441	62.387111
1938.045455	3532.367507	62.392116
1937.145356	3468.267569	62.397121
1936.730001	3412.535920	62.402126
1935.845503	3360.954737	62.407130
1935.352560	3298.776740	62.412135
1934.596915	3245.158923	62.417140
1933.732014	3197.558678	62.422145
1933.257612	3144.066930	62.427150
1932.424173	3082.460468	62.432154
1931.820857	3029.878401	62.437159
1930.902483	2976.084722	62.442164
1930.305847	2923.362389	62.447169
1929.793069	2881.301049	62.452174
1928.964617	2824.011849	62.457178
1928.602279	2768.999767	62.462183
1927.891787	2719.310369	62.467188
1927.365301	2676.224220	62.472193
1926.768352	2617.146764	62.477198
1926.133297	2548.512871	62.482202
1925.364345	2496.444014	62.487207
1924.313152	2459.519624	62.492212
1924.026241	2384.334678	62.497217
1923.486011	2344.026000	62.502222
1922.237327	2289.191132	62.507226
1921.716765	2238.409396	62.512231
1921.377943	2193.909313	62.517236
1920.332489	2140.860448	62.522241
1919.540182	2091.205890	62.527246
1918.988446	2034.712547	62.532250
1918.926164	1989.315935	62.537255
1917.577897	1943.989563	62.542260
1917.400191	1887.800945	62.547265
1916.642283	1838.394920	62.552270
1915.668400	1788.491853	62.557274
1915.459341	1738.688335	62.562279
1914.803155	1685.334874	62.567284
1913.603098	1634.208114	62.572289
1913.094596	1591.374653	62.577294
1912.379636	1544.224403	62.582298
1911.682843	1493.228787	62.587303
1911.010463	1457.586559	62.592308
1910.355330	1399.555487	62.597313
1909.926244	1347.941448	62.602318
1908.923421	1307.694095	62.607322
1908.562895	1251.895738	62.612327
1907.673428	1211.871949	62.617332
1907.380766	1154.809409	62.622337
1906.850230	1114.247897	62.627342
1905.860855	1075.465730	62.632346
1905.469102	1014.659744	62.637351
1904.568799	979.248066	62.642356
1903.573270	927.388747	62.647361
1902.965106	880.487852	62.652366
1902.014199	850.127918	62.657370
1901.601889	788.091319	62.662375
1900.911718	753.940001	62.667380
1899.908594	709.890556	62.672385
1899.572516	667.552073	62.677390
1898.866316	630.915048	62.682394
1898.384877	592.644915	62.687399
1897.452352	556.286872	62.692404
1896.808327	517.041350	62.697409
1896.382441	464.386751	62.702414
1895.284917	436.955012	62.707418
1894.760089	399.655824	62.712423
1894.244904	359.586007	62.717428
1893.351181	320.549400	62.722433
1892.830623	276.792097	62.727438
1891.939049	241.989555	62.732442
1891.182196	204.289308	62.737447
1890.620580	182.263202	62.742452
1889.881264	143.544762	62.747457
1889.290152	107.658774	62.752462
1888.132451	85.524027	62.757466
1887.641259	56.485233	62.762471
1886.560741	28.311194	62.767476
1885.884558	16.689351	62.772481
1884.863585	-7.619498	62.777486
1883.319841	-17.879856	62.782490
1881.926298	17.149600	62.787495
1880.795710	30.023752	62.792500
1880.432683	27.347129	62.797505
1880.203745	23.953781	62.802510
1879.442834	39.842730	62.807514
1879.883128	40.925753	62.812519
1879.234141	34.864655	62.817524
1878.255602	41.017354	62.822529
1877.312785	41.640310	62.827534
1876.624492	44.697097	62.832538
1875.841742	45.740918	62.837543
1875.472729	49.040327	62.842548
1874.887388	41.879446	62.847553
1874.571939	46.867153	62.852558
1873.284720	57.337689	62.857562
1872.871643	45.812826	62.862567
1872.091978	53.425755	62.867572
1871.935612	57.196029	62.872577
1871.764312	45.599662	62.877582
1870.219853	49.719639	62.882586
1869.588713	53.434408	62.887591
1869.066280	56.259860	62.892596
1868.545889	52.879666	62.897601
1868.061932	55.962361	62.902606
1866.934063	53.670527	62.907610
1866.309330	48.323091	62.912615
1865.488077	61.700094	62.917620
1864.916475	49.979626	62.922625
1864.096514	44.593804	62.927630
1863.811902	56.460029	62.932634
1863.859006	53.413932	62.937639
1862.573057	48.403297	62.942644
1861.648800	53.451403	62.947649
1861.441197	57.018500	62.952654
1861.057230	54.379893	62.957658
1859.973678	54.782351	62.962663
1858.883775	53.608861	62.967668
1859.100333	47.299946	62.972673
1858.264578	52.816549	62.977678
1856.989745	55.330961	62.982682
1856.688386	50.241265	62.987687
1856.337780	54.375118	62.992692
1855.440832	51.114642	62.997697
1854.734946	55.453141	63.002702
1853.816814	51.920061	63.007706
1853.873355	53.254826	63.012711
1852.183178	52.380079	63.017716
1852.096968	58.252335	63.022721
1851.681849	56.143802	63.027726
1850.936497	56.159825	63.032730
1850.328003	55.586413	63.037735
1849.323466	58.456880	63.042740
1848.453108	57.325805	63.047745
1848.282988	58.933104	63.052750
1847.547279	58.067655	63.057754
1847.358648	52.225199	63.062759
1845.747911	63.753217	63.067764
1845.136943	58.864070	63.072769
1845.133014	57.778347	63.077774
1844.499623	60.089988	63.082778
1843.259826	55.166650	63.087783
1842.837137	67.057962	63.092788
1842.591296	58.854422	63.097793
1841.476023	58.957572	63.102798
1840.351553	63.668471	63.107802
1840.711891	49.956569	63.112807
1839.396441	55.713351	63.117812
1839.137377	60.080253	63.122817
1838.283510	52.739665	63.127822
1837.382502	60.786613	63.132826
1836.990950	49.190530	63.137831
1836.266099	55.624664	63.142836
1835.695402	58.281167	63.147841
1835.093290	54.986497	63.152846
1833.978253	59.803133	63.157850
1833.933903	47.726142	63.162855
1833.388388	63.304952	63.167860
1832.648928	57.031143	63.172865
1832.093803	59.155318	63.177870
1831.667447	57.971092	63.182874
1830.929520	47.519689	63.187879
1829.662054	50.452413	63.192884
1828.380047	53.639760	63.197889
1828.457782	50.866344	63.202894
1828.031817	60.315468	63.207898
1827.016305	55.769686	63.212903
1826.265526	56.732751	63.217908
1825.702133	55.855716	63.222913
1825.182591	56.413055	63.227918
1824.373228	57.112610	63.232922
1824.163612	58.207362	63.237927
1823.282758	58.891462	63.242932
1822.463386	59.206253	63.247937
1822.333583	46.474205	63.252942
1821.444368	52.373045	63.257946
1821.173222	58.907025	63.262951
1820.442374	60.228050	63.267956
1819.305702	53.791818	63.272961
1818.614033	51.181581	63.277966
1817.758612	60.703632	63.282970
1817.320276	49.094483	63.287975
1816.355202	57.280918	63.292980
1816.065735	52.985703	63.297985
1815.622915	50.047367	63.302990
1814.797455	55.917162	63.307994
1814.112954	49.951604	63.312999
1812.879463	57.046834	63.318004
1812.661103	58.340095	63.323009
1812.029323	50.959521	63.328014
1811.262377	59.105034	63.333018
1810.420759	46.536486	63.338023
1809.674073	49.525292	63.343028
1809.317402	47.457949	63.348033
1808.875536	50.576546	63.353038
1808.143823	62.644661	63.358042
1807.742545	54.079459	63.363047
1807.394437	58.345385	63.368052
1806.723083	54.927677	63.373057
1805.831044	49.687362	63.378062
1804.576422	58.402329	63.383066
1804.135626	52.451690	63.388071
1803.702173	53.432178	63.393076
1802.883096	60.942575	63.398081
1802.642909	49.883861	63.403086
1801.498023	49.884497	63.408090
1800.405188	51.343435	63.413095
1799.593094	54.528712	63.418100
1799.702454	51.753427	63.423105
1799.107617	49.496825	63.428110
1798.078937	55.256971	63.433114
1797.628376	49.191190	63.438119
1797.123681	53.556099	63.443124
1796.540196	50.925534	63.448129
1795.933191	52.807217	63.453134
1794.741093	55.944032	63.458138
1794.398006	43.934991	63.463143
1793.759031	53.805870	63.468148
1793.297953	55.602879	63.473153
1792.879118	48.180611	63.478158
1791.451346	51.108848	63.483162
1790.524769	52.278036	63.488167
1789.911034	53.190963	63.493172
1789.383553	56.638550	63.498177
1788.994703	56.093351	63.503182
1788.017854	50.040187	63.508186
1787.851583	41.568564	63.513191
1787.374740	47.360923	63.518196
1786.581992	51.227528	63.523201
1786.703940	46.171547	63.528206
1784.774636	55.868874	63.533210
1784.267295	55.596382	63.538215
1783.376777	60.095106	63.543220
1782.811077	54.257347	63.548225
1782.750834	48.859714	63.553230
1781.763686	57.855488	63.558234
1781.429600	55.289398	63.563239
1780.857284	56.998419	63.568244
1779.636146	59.509071	63.573249
1779.231171	49.200354	63.578254
1778.492782	57.295606	63.583258
1778.018780	52.607079	63.588263
1777.109916	49.480990	63.593268
1776.335998	53.536996	63.598273
1775.715477	62.957098	63.603278
1774.949713	65.873252	63.608282
1774.317141	61.815456	63.613287
1773.820265	65.663466	63.618292
1773.151905	64.175484	63.623297
1772.939441	62.853220	63.628302
1771.726075	60.537158	63.633306
1771.413709	63.067493	63.638311
1771.054536	56.223955	63.643316
1770.073838	57.436439	63.648321
1769.320682	58.723173	63.653326
1768.332342	55.351088	63.658330
1767.868736	59.859287	63.663335
1767.678682	56.338345	63.668340
1766.929930	61.552575	63.673345
1765.871376	53.799822	63.678350
1764.970919	53.614998	63.683354
1764.549326	64.194110	63.688359
1764.009666	60.717651	63.693364
1763.467260	58.916355	63.698369
1762.999863	61.723624	63.703374
1762.034670	57.578310	63.708378
1761.338224	60.764155	63.713383
1760.385145	56.329913	63.718388
1759.958840	66.599115	63.723393
1759.748299	62.393873	63.728398
1758.754280	65.858792	63.733402
1757.819483	54.290657	63.738407
1756.930919	59.814099	63.743412
1756.128219	62.833894	63.748417
1755.774629	56.303287	63.753422
1755.612654	63.786607	63.758426
1755.287846	62.195182	63.763431
1754.761118	62.829370	63.768436
1754.008146	68.939986	63.773441
1753.062581	45.104861	63.778446
1752.124830	56.740501	63.783450
1751.780297	50.195844	63.788455
1750.184946	61.831851	63.793460
1749.463883	54.482822	63.798465
1749.486796	55.051793	63.803470
1748.755549	56.294053	63.808474
1748.342593	59.458530	63.813479
1747.657113	56.710135	63.818484
1746.975304	65.207996	63.823489
1746.799397	55.853230	63.828494
1745.055539	57.969099	63.833498
1744.454296	60.789744	63.838503
1743.909162	55.145849	63.843508
1743.282350	57.508506	63.848513
1743.119513	58.229982	63.853518
1742.351299	52.678288	63.858522
1742.096180	48.224666	63.863527
1740.916499	63.726005	63.868532
1739.817371	58.004517	63.873537
1739.527641	41.901131	63.878542
1739.032844	53.985237	63.883546
1738.775367	53.111674	63.888551
1737.760334	53.170562	63.893556
1736.836052	47.661006	63.898561
1736.339342	41.500071	63.903566
1735.350241	52.074694	63.908570
1735.375340	44.350122	63.913575
1734.750691	60.916058	63.918580
1733.459347	56.526090	63.923585
1732.798508	42.689383	63.928590
1731.982413	63.100377	63.933594
1731.476277	50.089070	63.938599
1730.863051	49.374513	63.943604
1730.627120	53.837093	63.948609
1730.255449	48.665547	63.953614
1728.902610	54.130271	63.958618
1728.337205	41.334968	63.963623
1727.496376	47.614077	63.968628
1726.982807	52.735766	63.973633
1726.799711	48.089357	63.978638
1725.852804	54.569821	63.983642
1725.215917	56.140875	63.988647
1724.613230	54.432741	63.993652
1724.071937	51.797070	63.998657
1723.535168	42.931718	64.003662
1722.043129	54.693249	64.008666
1721.692308	47.832630	64.013671
1721.306480	51.081110	64.018676
1720.767778	45.160236	64.023681
1719.778757	48.312134	64.028686
1718.721774	51.161014	64.033690
1718.546059	49.659455	64.038695
1717.541989	49.503721	64.043700
1717.099950	52.075155	64.048705
1717.071467	47.132954	64.053710
1716.241281	61.654692	64.058714
1714.962683	43.186828	64.063719
1714.496062	43.816207	64.068724
1713.782654	54.391202	64.073729
1713.544223	42.773992	64.078734
1712.201750	55.795411	64.083738
1711.822801	44.927494	64.088743
1710.813259	59.979190	64.093748
1710.641421	52.618633	64.098753
1710.118177	57.558936	64.103758
1709.315229	47.046947	64.108762
1709.058797	54.005946	64.113767
1707.787475	41.412663	64.118772
1706.783383	53.848902	64.123777
1706.506247	44.901314	64.128782
1705.842476	57.475888	64.133786
1705.327923	49.896957	64.138791
1705.031591	56.972682	64.143796
1703.900167	55.193996	64.148801
1703.098883	40.971180	64.153806
1702.368363	65.115424	64.158810
1702.065671	47.620073	64.163815
1701.676013	63.596755	64.168820
1701.097951	55.837098	64.173825
1700.240718	57.353271	64.178830
1699.232361	62.646600	64.183834
1698.952537	52.817918	64.188839
1698.124274	59.607553	64.193844
1697.114861	55.947107	64.198849
1696.797917	47.622431	64.203854
1696.051257	52.099905	64.208858
1695.980545	47.695846	64.213863
1694.706537	48.060815	64.218868
1693.437695	53.679369	64.223873
1692.939961	42.459744	64.228878
1692.704552	50.580770	64.233882
1692.329191	46.176217	64.238887
1691.414165	54.468276	64.243892
1691.303226	48.809045	64.248897
1690.071529	54.803323	64.253902
1689.300429	50.953640	64.258906
1688.625738	57.799307	64.263911
1688.259787	52.841326	64.268916
1687.780998	51.512490	64.273921
1686.819588	51.747383	64.278926
1685.817907	52.047021	64.283930
1685.449143	56.959635	64.288935
1684.808536	57.600887	64.293940
1684.617674	54.231470	64.298945
1684.029318	59.686744	64.303950
1682.809086	55.249239	64.308954
1682.638281	50.108874	64.313959
1681.347062	58.694084	64.318964
1680.225461	57.249739	64.323969
1679.930252	57.727317	64.328974
1679.021762	52.503857	64.333978
1679.032968	54.621678	64.338983
1678.485723	50.072542	64.343988
1677.843153	58.091093	64.348993
1677.661986	47.511887	64.353998
1676.444444	50.277478	64.359002
1675.996615	59.326383	64.364007
1674.900262	51.414101	64.369012
1673.450315	55.533367	64.374017
1673.320722	55.144121	64.379022
1672.337647	49.790588	64.384026
1672.279396	53.270889	64.389031
1672.110613	48.196436	64.394036
1671.852032	57.268895	64.399041
1670.665106	45.444394	64.404046
1669.123935	59.717956	64.409050
1668.811188	56.948221	64.414055
1668.291639	55.280511	64.419060
1667.569795	52.864346	64.424065
1667.381433	54.450895	64.429070
1665.890663	60.208797	64.434074
1665.464836	44.678982	64.439079
1664.722858	59.107866	64.444084
1664.284495	53.871232	64.449089
1664.294422	43.618067	64.454094
1663.260732	47.877792	64.459098
1662.102057	49.334630	64.464103
1661.539721	48.471657	64.469108
1660.785867	49.206598	64.474113
1660.343057	50.726336	64.479118
1659.625313	43.403626	64.484122
1659.594483	35.197517	64.489127
1658.755140	46.062179	64.494132
1657.991378	46.283031	64.499137
1657.568678	48.442971	64.504142
1656.298812	49.900128	64.509146
1655.705993	57.320998	64.514151
1655.039294	57.274119	64.519156
1654.369950	53.778867	64.524161
1654.156731	53.251519	64.529166
1652.825469	58.222420	64.534170
1652.181580	49.135983	64.539175
1651.392836	56.165354	64.544180
1650.998449	59.612323	64.549185
1651.110112	55.045252	64.554190
1650.341970	53.879085	64.559194
1648.992288	58.829259	64.564199
1648.089077	49.022352	64.569204
1647.676905	56.419255	64.574209
1647.446510	51.458671	64.579214
1646.751679	51.808925	64.584218
1646.075866	46.357707	64.589223
1645.345233	47.481625	64.594228
1644.782110	55.996913	64.599233
1644.482773	40.454900	64.604238
1643.065207	56.306286	64.609242
1642.413461	43.023258	64.614247
1641.919165	51.746806	64.619252
1641.366959	59.288960	64.624257
1640.970762	46.864195	64.629262
1639.503305	49.436116	64.634266
1638.764388	54.457999	64.639271
1638.435005	43.416649	64.644276
1637.755971	51.612882	64.649281
1637.904658	41.302985	64.654286
1636.730991	52.733277	64.659290
1636.028325	52.597501	64.664295
1634.995672	46.270997	64.669300
1634.718083	53.152934	64.674305
1634.621196	35.599693	64.679310
1633.501971	54.748395	64.684314
1632.701958	41.701816	64.689319
1632.154316	54.819342	64.694324
1631.506278	44.702248	64.699329
1630.561636	44.363641	64.704334
1629.721306	53.875448	64.709338
1629.326045	43.193072	64.714343
1628.648968	49.734774	64.719348
1628.508911	56.558593	64.724353
1627.681687	58.667687	64.729358
1626.495775	56.446684	64.734362
1626.024668	48.772565	64.739367
1625.482642	50.932543	64.744372
1624.799821	53.146428	64.749377
1624.352311	44.549199	64.754382
1622.987192	62.694615	64.759386
1623.125225	54.203052	64.764391
1621.993230	49.934488	64.769396
1621.807783	57.766883	64.774401
1621.225100	59.375081	64.779406
1620.159972	53.299746	64.784410
1619.898705	51.661977	64.789415
1619.133510	50.020689	64.794420
1618.253002	58.335670	64.799425
1617.486649	51.623089	64.804430
1616.902393	46.936349	64.809434
1615.981236	53.442715	64.814439
1615.116086	52.818673	64.819444
1614.294132	55.767448	64.824449
1614.389803	52.382479	64.829454
1613.586862	51.398471	64.834458
1613.142748	43.305330	64.839463
1612.698999	48.340247	64.844468
1611.705325	55.958849	64.849473
1610.968717	54.593719	64.854478
1610.243222	51.938454	64.859482
1609.640376	47.488058	64.864487
1608.907965	47.861639	64.869492
1607.696074	45.452387	64.874497
1607.644749	52.777769	64.879502
1607.011705	60.525160	64.884506
1606.846914	52.012324	64.889511
1605.549762	53.849155	64.894516
1604.751800	49.751456	64.899521
1604.605644	52.796292	64.904526
1603.758050	58.627080	64.909530
1602.684024	46.339981	64.914535
1601.735818	58.533982	64.919540
1601.241314	57.840018	64.924545
1600.910338	46.240687	64.929550
1600.527945	52.866463	64.934554
1600.400025	53.155045	64.939559
1599.323038	47.258225	64.944564
1597.982619	53.834363	64.949569
1597.694562	52.440549	64.954574
1597.251405	59.760380	64.959578
1596.552968	50.406661	64.964583
1595.703652	57.677481	64.969588
1594.886202	62.054266	64.974593
1594.842189	49.603519	64.979598
1593.725280	50.176965	64.984602
1593.035215	46.815912	64.989607
1592.637086	44.990157	64.994612
1592.177845	47.485493	64.999617
1591.175454	48.638410	65.004622
1589.999755	51.924093	65.009626
1589.769196	44.870931	65.014631
1589.033142	54.030289	65.019636
1588.844421	53.212050	65.024641
1587.998105	37.357994	65.029646
1587.089830	50.119657	65.034650
1586.501647	44.116796	65.039655
1585.958287	49.773092	65.044660
1584.639456	46.830486	65.049665
1583.775225	47.592447	65.054670
1583.430775	58.958820	65.059674
1583.440439	45.994925	65.064679
1582.802275	53.585434	65.069684
1581.891575	53.287184	65.074689
1582.157994	47.883398	65.079694
1580.611320	62.630962	65.084698
1580.196704	47.920983	65.089703
1578.880525	53.476145	65.094708
1578.122385	53.295582	65.099713
1577.713239	49.577662	65.104718
1577.222456	49.591162	65.109722
1577.128035	45.772775	65.114727
1575.802091	47.519577	65.119732
1574.813871	46.025703	65.124737
1574.627738	32.613538	65.129742
1573.888444	47.422040	65.134746
1573.434025	43.947857	65.139751
1573.182264	44.199347	65.144756
1572.165097	52.406740	65.149761
1571.821588	46.850707	65.154766
1570.747587	48.573250	65.159770
1569.673226	32.208241	65.164775
1568.951111	39.673313	65.169780
1568.330688	50.315555	65.174785
1568.426415	43.071782	65.179790
1567.557199	47.187137	65.184794
1566.508658	43.946129	65.189799
1565.735056	45.540518	65.194804
1565.312047	41.129370	65.199809
1564.775674	42.537832	65.204814
1564.465494	48.663281	65.209818
1563.374573	44.410299	65.214823
1562.622342	38.510784	65.219828
1562.281767	44.704138	65.224833
1561.768741	48.668282	65.229838
1560.594158	47.527300	65.234842
1559.997557	37.047250	65.239847
1559.476693	45.440711	65.244852
1559.076202	38.638486	65.249857
1557.886492	41.806558	65.254862
1557.035893	55.103114	65.259866
1556.943192	48.701409	65.264871
1556.254173	45.895287	65.269876
1555.595243	47.845196	65.274881
1554.529370	42.411833	65.279886
1553.907782	49.942941	65.284890
1553.257742	42.790861	65.289895
1553.071875	46.422324	65.294900
1552.278449	42.120499	65.299905
1551.946845	40.351990	65.304910
1550.649083	43.882586	65.309914
1550.336485	37.561560	65.314919
1549.677453	48.408633	65.319924
1548.554248	40.421841	65.324929
1548.112218	43.160453	65.329934
1547.683736	51.473007	65.334938
1547.380438	43.499434	65.339943
1546.053420	47.299609	65.344948
1545.103059	44.069818	65.349953
1544.950836	36.513789	65.354958
1544.293150	45.980818	65.359962
1544.000003	43.144912	65.364967
1542.757774	46.538955	65.369972
1541.866166	42.564971	65.374977
1541.875550	34.997457	65.379982
1540.855858	44.887860	65.384986
1540.447984	44.380416	65.389991
1539.237817	43.363370	65.394996
1538.627585	48.703870	65.400001
1538.535620	44.314240	65.405006
1537.942924	42.975150	65.410010
1537.158247	35.489660	65.415015
1536.392137	40.891197	65.420020
1535.470373	40.414950	65.425025
1535.421335	34.369014	65.430030
1534.302672	48.879837	65.435034
1533.537997	46.538329	65.440039
1532.882956	44.620945	65.445044
1532.159235	42.378585	65.450049
1532.161406	46.360213	65.455054
1530.720915	48.320781	65.460058
1530.200327	42.168425	65.465063
1529.942734	51.373186	65.470068
1529.178831	49.141942	65.475073
1528.292596	48.964403	65.480078
1527.218827	42.762757	65.485082
1526.803526	48.598984	65.490087
1526.678926	36.503262	65.495092
1526.130809	44.122044	65.500097
1525.046880	37.185581	65.505102
1524.031666	44.203655	65.510106
1523.596713	41.926449	65.515111
1523.333002	46.130099	65.520116
1522.519029	41.527199	65.525121
1522.251361	39.300681	65.530126
1521.249005	43.022467	65.535130
1520.964972	34.530181	65.540135
1519.774693	43.399027	65.545140
1518.584059	44.122993	65.550145
1518.481509	36.530689	65.555150
1517.997928	48.313401	65.560154
1517.268566	39.201176	65.565159
1516.130210	50.217465	65.570164
1515.735036	34.927268	65.575169
1515.553008	50.213347	65.580174
1514.820869	40.978562	65.585178
1514.066332	35.864752	65.590183
1512.977849	47.152234	65.595188
1512.470296	46.823060	65.600193
1512.282647	38.326495	65.605198
1511.218633	51.081385	65.610202
1510.394904	42.728477	65.615207
1510.026548	45.851201	65.620212
1509.357138	44.128495	65.625217
1508.537424	35.923187	65.630222
1507.503710	48.163906	65.635226
1506.934756	39.008848	65.640231
1506.504759	37.380561	65.645236
1506.011422	38.536191	65.650241
1505.876235	40.025989	65.655246
1504.800280	39.883339	65.660250
1504.180862	38.245730	65.665255
1503.342143	42.107098	65.670260
1502.466699	41.981469	65.675265
1502.001603	43.854854	65.680270
1501.108942	38.764575	65.685274
1501.184532	38.979819	65.690279
1500.157462	42.478460	65.695284
1499.017143	44.875465	65.700289
1498.512025	33.478887	65.705294
1498.066894	43.639115	65.710298
1497.554630	43.697045	65.715303
1496.579613	46.020473	65.720308
1495.796491	43.366519	65.725313
1495.591317	44.061620	65.730318
1494.969378	41.336320	65.735322
1494.050569	34.312131	65.740327
1493.157779	40.055508	65.745332
1492.770763	41.702021	65.750337
1492.203727	35.323671	65.755342
1491.309027	34.040473	65.760346
1490.470313	40.495921	65.765351
1489.670939	40.154782	65.770356
1489.549331	38.486950	65.775361
1489.612239	50.454051	65.780366
1488.361544	41.935618	65.785370
1487.500556	48.001950	65.790375
1487.098499	43.265791	65.795380
1485.694432	46.026415	65.800385
1484.960649	39.521602	65.805390
1484.346240	41.609530	65.810394
1484.137752	41.141370	65.815399
1483.774105	39.097267	65.820404
1483.326427	47.595801	65.825409
1482.214635	42.384235	65.830414
1481.076049	52.314056	65.835418
1481.112685	42.586523	65.840423
1480.621984	39.261630	65.845428
1479.410491	51.596844	65.850433
1479.153614	44.328688	65.855438
1478.198039	51.551767	65.860442
1477.741400	43.839120	65.865447
1476.719720	44.402213	65.870452
1476.090723	46.285882	65.875457
1475.882569	40.361430	65.880462
1474.730827	56.017667	65.885466
1474.196756	47.010035	65.890471
1473.545859	44.205764	65.895476
1472.914764	48.048337	65.900481
1472.705503	42.565606	65.905486
1471.317430	49.882653	65.910490
1470.709355	45.570322	65.915495
1470.368199	35.589024	65.920500
1469.884144	43.369519	65.925505
1469.146863	38.565217	65.930510
1468.019357	36.836481	65.935514
1467.569891	39.424898	65.940519
1467.165822	45.278268	65.945524
1466.233660	45.100165	65.950529
1465.509828	42.307489	65.955534
1464.745394	46.382565	65.960538
1464.730430	37.815986	65.965543
1464.201680	43.785365	65.970548
1463.069416	44.979471	65.975553
1462.909491	39.296514	65.980558
1461.207659	47.656908	65.985562
1460.472968	30.924169	65.990567
1459.837086	39.004758	65.995572
1459.416738	39.125358	66.000577
1459.089363	51.780532	66.005582
1458.375756	40.382404	66.010586
1458.431664	31.878682	66.015591
1457.447647	44.526250	66.020596
1456.217601	48.634330	66.025601
1456.034850	35.937585	66.030606
1455.285190	40.063931	66.035610
1454.063446	44.664276	66.040615
1453.640105	35.061896	66.045620
1453.179935	37.171048	66.050625
1452.924049	32.200357	66.055630
1451.417954	42.265862	66.060634
1450.621245	41.951119	66.065639
1450.189185	46.197299	66.070644
1449.960965	43.409434	66.075649
1449.833422	35.884190	66.080654
1448.317283	52.524015	66.085658
1447.918992	41.012697	66.090663
1447.460730	47.089148	66.095668
1446.305878	44.212018	66.100673
1445.510991	54.221266	66.105678
1444.353234	50.802128	66.110682
1444.504224	42.297480	66.115687
1444.270830	44.258628	66.120692
1443.622438	47.807489	66.125697
1442.874555	51.824749	66.130702
1441.972106	46.616199	66.135706
1441.478461	42.372422	66.140711
1440.730691	51.205662	66.145716
1439.454840	47.314866	66.150721
1439.258084	46.560995	66.155726
1438.781073	46.935030	66.160730
1438.144692	43.500838	66.165735
1437.006987	50.774953	66.170740
1436.164019	46.160922	66.175745
1435.907971	39.621195	66.180750
1435.592235	49.005506	66.185754
1434.826035	37.997370	66.190759
1433.776483	45.249588	66.195764
1433.261449	46.757186	66.200769
1432.921994	48.001912	66.205774
1431.719539	41.057524	66.210778
1431.411707	46.551827	66.215783
1430.827900	48.579710	66.220788
1430.222270	42.693209	66.225793
1429.469949	38.022199	66.230798
1428.469037	49.253211	66.235802
1428.046203	47.696338	66.240807
1427.697751	49.552773	66.245812
1426.196096	49.574012	66.250817
1425.778684	42.916431	66.255822
1425.107743	50.335556	66.260826
1425.246681	40.812541	66.265831
1424.553816	41.716050	66.270836
1423.123056	43.651474	66.275841
1422.809284	45.756286	66.280846
1422.257126	44.588976	66.285850
1421.596559	46.250595	66.290855
1420.655291	49.775051	66.295860
1419.850462	50.854053	66.300865
1419.743420	46.458944	66.305870
1418.672079	47.782157	66.310874
1417.902308	47.292832	66.315879
1417.258353	52.375365	66.320884
1416.577517	50.014260	66.325889
1416.290828	35.941600	66.330894
1415.879656	45.330040	66.335898
1414.728817	42.977411	66.340903
1414.051208	56.233883	66.345908
1413.198266	52.040912	66.350913
1413.463269	47.684437	66.355918
1412.074879	55.750615	66.360922
1411.742352	42.850600	66.365927
1411.187874	46.505966	66.370932
1409.868760	44.009777	66.375937
1409.754461	43.793156	66.380942
1408.846467	53.519192	66.385946
1408.265870	39.650943	66.390951
1407.024488	42.966064	66.395956
1406.308605	45.978461	66.400961
1406.039025	42.645245	66.405966
1405.468755	55.362684	66.410970
1405.005494	42.529184	66.415975
1404.908987	43.918221	66.420980
1403.477363	49.329385	66.425985
1403.067363	42.721093	66.430990
1402.545508	45.421953	66.435994
1402.052963	45.312765	66.440999
1400.741107	45.608200	66.446004
1399.885379	54.452302	66.451009
1399.826447	46.096141	66.456014
1399.050970	54.410248	66.461018
1397.840600	44.382626	66.466023
1397.483323	49.791752	66.471028
1397.192580	49.372944	66.476033
1396.680253	45.121108	66.481038
1395.499043	53.021895	66.486042
1395.083941	47.970861	66.491047
1394.469404	44.643594	66.496052
1393.825090	46.709489	66.501057
1393.143818	43.320291	66.506062
1391.973034	53.469725	66.511066
1391.571832	42.274275	66.516071
1391.197567	44.891751	66.521076
1390.288073	46.520407	66.526081
1389.609459	40.992449	66.531086
1388.768395	53.793935	66.536090
1388.257012	39.468416	66.541095
1388.277693	42.090920	66.546100
1387.094738	49.017432	66.551105
1386.520313	50.766291	66.556110
1385.861046	51.334888	66.561114
1385.382343	47.101364	66.566119
1384.395857	46.263300	66.571124
1383.921803	49.891694	66.576129
1383.165714	40.135644	66.581134
1381.777602	34.581704	66.586138
1381.256571	44.225728	66.591143
1381.184697	40.593007	66.596148
1380.531988	36.849192	66.601153
1380.145155	41.174922	66.606158
1379.548187	44.226769	66.611162
1379.025539	44.538684	66.616167
1378.043458	41.440160	66.621172
1376.742015	51.750716	66.626177
1376.452021	46.537874	66.631182
1375.581668	38.662366	66.636186
1375.003163	36.114698	66.641191
1374.676740	47.000383	66.646196
1373.805417	44.335259	66.651201
1373.207861	38.387570	66.656206
1372.304732	51.033344	66.661210
1372.066357	42.726213	66.666215
1371.673603	46.748536	66.671220
1370.771124	44.768030	66.676225
1369.970955	47.913683	66.681230
1369.258072	55.358411	66.686234
1368.510416	42.257897	66.691239
1367.628482	47.040802	66.696244
1366.783724	46.397834	66.701249
1366.631837	42.361519	66.706254
1366.100121	37.868349	66.711258
1365.826368	39.736569	66.716263
1364.773334	38.775053	66.721268
1364.304976	45.665244	66.726273
1363.204498	33.442417	66.731278
1362.265664	46.909146	66.736282
1361.585748	37.976779	66.741287
1361.443206	41.514627	66.746292
1361.108462	48.298423	66.751297
1360.265805	47.013306	66.756302
1359.260121	42.021475	66.761306
1359.094120	40.144667	66.766311
1357.684571	39.507911	66.771316
1356.374948	39.536510	66.776321
1356.006762	47.361676	66.781326
1355.707741	45.963329	66.786330
1355.604430	40.955779	66.791335
1355.313336	38.720391	66.796340
1354.394955	44.860536	66.801345
1353.929089	40.580826	66.806350
1353.120062	46.123271	66.811354
1352.168099	42.349767	66.816359
1350.978122	44.865115	66.821364
1350.385165	49.475930	66.826369
1350.201312	33.707494	66.831374
1349.639962	40.699200	66.836378
1348.672202	38.557194	66.841383
1347.875231	42.013002	66.846388
1347.274196	45.229504	66.851393
1347.199504	48.378100	66.856398
1345.943228	45.917687	66.861402
1345.351559	41.161240	66.866407
1344.596372	42.771688	66.871412
1344.327344	51.196101	66.876417
1344.014555	42.151757	66.881422
1342.856727	50.048845	66.886426
1342.181437	46.663442	66.891431
1342.140370	40.444365	66.896436
1340.578047	42.569483	66.901441
1340.149528	37.621522	66.906446
1339.582793	46.627847	66.911450
1338.897625	42.099154	66.916455
1338.151737	39.601759	66.921460
1336.916316	46.000470	66.926465
1336.898737	34.600550	66.931470
1336.242395	39.781257	66.936474
1336.031640	42.464208	66.941479
1334.925004	38.672724	66.946484
1334.089821	45.540812	66.951489
1334.017502	38.278037	66.956494
1332.419240	44.734434	66.961498
1331.841210	42.358587	66.966503
1331.402485	45.470441	66.971508
1330.555001	43.086971	66.976513
1330.931223	41.855664	66.981518
1329.830830	42.316211	66.986522
1328.794235	39.819306	66.991527
1328.387202	43.943250	66.996532
1327.902206	42.101391	67.001537
1327.521769	41.299461	67.006542
1326.473993	49.565410	67.011546
1325.818579	38.522360	67.016551
1325.015348	42.975799	67.021556
1323.868635	45.438548	67.026561
1323.921869	37.192300	67.031566
1323.368420	43.540938	67.036570
1322.465181	46.291408	67.041575
1321.419548	38.338135	67.046580
1320.431382	53.763403	67.051585
1320.430371	44.565415	67.056590
1319.929579	47.464789	67.061594
1318.857956	39.211299	67.066599
1317.958143	52.326488	67.071604
1317.496999	53.486496	67.076609
1317.645404	40.634626	67.081614
1316.880913	44.780711	67.086618
1315.751892	37.913022	67.091623
1315.155796	48.746967	67.096628
1314.267700	45.385945	67.101633
1313.678750	34.854304	67.106638
1312.551559	49.448546	67.111642
1312.246519	38.080138	67.116647
1312.184491	43.161630	67.121652
1311.519070	43.663416	67.126657
1310.353672	43.587106	67.131662
1309.319468	48.233390	67.136666
1309.268739	38.679037	67.141671
1308.674740	50.720591	67.146676
1308.090759	40.142427	67.151681
1307.396369	42.378727	67.156686
1306.617496	44.207416	67.161690
1305.909433	41.737133	67.166695
1304.845761	38.351992	67.171700
1304.048458	48.274916	67.176705
1304.098330	35.186407	67.181710
1303.489762	43.278449	67.186714
1302.587966	39.697262	67.191719
1301.804551	37.281540	67.196724
1301.096090	40.414206	67.201729
1301.043675	29.697920	67.206734
1299.930502	44.297816	67.211738
1299.500347	32.715920	67.216743
1299.194821	35.776636	67.221748
1297.679741	47.075239	67.226753
1296.872167	34.782225	67.231758
1296.517865	44.759291	67.236762
1295.825261	46.858116	67.241767
1295.740050	34.969063	67.246772
1294.454798	44.862337	67.251777
1294.131355	39.727369	67.256782
1293.325703	40.681961	67.261786
1292.642793	33.700778	67.266791
1291.537198	35.680765	67.271796
1290.791608	39.320805	67.276801
1290.548070	24.787169	67.281806
1290.089021	38.418893	67.286810
1289.530697	28.166246	67.291815
1288.743172	40.153408	67.296820
1287.994446	38.643648	67.301825
1287.681799	35.164335	67.306830
1286.485290	45.932898	67.311834
1285.458223	36.313016	67.316839
1285.050150	38.483296	67.321844
1284.416858	43.844853	67.326849
1284.627320	38.642342	67.331854
1283.827830	40.267735	67.336858
1282.722296	34.198995	67.341863
1282.173696	40.270901	67.346868
1281.508182	38.650142	67.351873
1280.881533	35.211295	67.356878
1279.830783	42.310789	67.361882
1279.192097	34.792725	67.366887
1278.694828	46.845706	67.371892
1278.474053	36.932044	67.376897
1277.870074	40.101719	67.381902
1276.843742	39.389882	67.386906
1276.267947	44.526257	67.391911
1275.080421	31.908894	67.396916
1274.087511	38.270644	67.401921
1273.946421	34.779823	67.406926
1273.591478	45.195383	67.411930
1273.195131	39.575273	67.416935
1272.060658	47.711521	67.421940
1271.322772	39.837072	67.426945
1271.278932	34.753844	67.431950
1270.417514	37.295831	67.436954
1269.306746	39.319228	67.441959
1268.749155	39.866955	67.446964
1268.061169	34.559725	67.451969
1267.967677	40.827349	67.456974
1266.513355	46.171227	67.461978
1266.145480	32.174598	67.466983
1265.843547	49.127623	67.471988
1265.095973	45.439926	67.476993
1264.077955	40.338136	67.481998
1263.096927	36.258634	67.487002
1263.119423	49.745991	67.492007
1262.945822	29.172578	67.497012
1261.721593	35.129568	67.502017
1260.727918	27.912387	67.507022
1259.848854	30.621183	67.512026
1259.562869	37.695269	67.517031
1259.431738	25.960188	67.522036
1258.183637	34.024616	67.527041
1257.607729	27.045357	67.532046
1256.889179	37.124493	67.537050
1256.502307	39.546871	67.542055
1255.934207	33.151414	67.547060
1255.286346	32.261134	67.552065
1254.482830	29.080654	67.557070
1253.410488	23.927589	67.562074
1252.620899	33.150702	67.567079
1252.742681	35.731892	67.572084
1251.675212	36.239276	67.577089
1250.993105	22.773596	67.582094
1250.081873	31.527199	67.587098
1249.660339	22.624758	67.592103
1249.431465	29.394871	67.597108
1248.232513	28.240567	67.602113
1248.032572	22.802125	67.607118
1247.084098	35.303736	67.612122
1246.177694	28.719230	67.617127
1245.533526	27.263821	67.622132
1244.629699	37.873889	67.627137
1244.245183	27.478503	67.632142
1244.123166	37.923250	67.637146
1243.522944	31.286902	67.642151
1242.613475	28.142198	67.647156
1241.534073	39.406233	67.652161
1241.719891	24.939952	67.657166
1240.363361	30.730331	67.662170
1239.169128	26.265279	67.667175
1239.263621	26.769243	67.672180
1238.868688	30.940156	67.677185
1237.606299	35.510784	67.682190
1236.856228	40.797879	67.687194
1236.266429	36.399134	67.692199
1235.875134	28.870132	67.697204
1235.461507	42.157172	67.702209
1234.900654	24.912782	67.707214
1233.929387	42.942055	67.712218
1233.502790	28.765544	67.717223
1232.361876	34.750298	67.722228
1231.179682	33.229063	67.727233
1231.329057	33.656491	67.732238
1230.572705	29.911858	67.737242
1230.117002	29.470418	67.742247
1229.294911	39.156020	67.747252
1228.270512	30.481913	67.752257
1228.158289	38.507649	67.757262
1227.407047	29.526755	67.762266
1226.290871	30.967560	67.767271
1225.805439	30.948738	67.772276
1225.326531	36.549102	67.777281
1225.229693	19.409127	67.782286
1223.945150	41.615074	67.787290
1223.008814	36.593355	67.792295
1222.883375	39.229627	67.797300
1221.871733	36.099600	67.802305
1221.086035	25.436862	67.807310
1220.459919	42.687432	67.812314
1220.154137	38.959457	67.817319
1220.007851	34.127490	67.822324
1218.486373	37.208118	67.827329
1218.134878	40.129497	67.832334
1217.326286	40.009104	67.837338
1216.799117	35.080014	67.842343
1215.961227	36.583801	67.847348
1214.853629	34.465665	67.852353
1214.483873	26.633625	67.857358
1214.306069	38.566414	67.862362
1213.570667	32.979739	67.867367
1212.891230	33.736089	67.872372
1212.349017	29.927446	67.877377
1211.486118	25.969531	67.882382
1210.338304	40.822537	67.887386
1209.989824	37.348934	67.892391
1209.888425	32.096671	67.897396
1208.417577	25.587755	67.902401
1207.881856	27.467686	67.907406
1207.077508	29.067066	67.912410
1206.797649	39.420219	67.917415
1206.506146	30.222718	67.922420
1205.587332	36.027083	67.927425
1204.708478	28.410048	67.932430
1204.264708	37.294327	67.937434
1203.783068	40.326290	67.942439
1202.485122	22.387013	67.947444
1201.875179	36.954206	67.952449
1201.560795	29.584868	67.957454
1200.762364	43.352573	67.962458
1200.310508	35.990902	67.967463
1199.456796	38.683071	67.972468
1198.354189	45.940651	67.977473
1198.583885	30.617416	67.982478
1197.649890	36.567700	67.987482
1196.861093	28.952115	67.992487
1196.411859	26.316127	67.997492
1195.682562	32.700630	68.002497
1195.624324	25.296866	68.007502
1194.247891	32.173792	68.012506
1193.734829	31.419785	68.017511
1192.716686	28.544693	68.022516
1191.601178	23.819567	68.027521
1191.385316	22.794369	68.032526
1190.680883	36.176539	68.037530
1190.474896	29.490126	68.042535
1189.977781	33.108019	68.047540
1188.823482	30.163121	68.052545
1188.426155	37.557690	68.057550
1187.815860	40.974391	68.062554
1187.150588	28.520029	68.067559
1186.482949	27.713337	68.072564
1185.790896	38.490011	68.077569
1184.737557	31.388008	68.082574
1183.572816	31.314806	68.087578
1183.093655	26.362323	68.092583
1182.546814	29.743699	68.097588
1182.153894	34.207609	68.102593
1182.091219	31.057563	68.107598
1181.522382	36.162882	68.112602
1180.795053	31.626756	68.117607
1180.209007	34.921329	68.122612
1178.703909	43.599098	68.127617
1178.031854	33.430804	68.132622
1177.602628	35.281190	68.137626
1176.937833	25.898641	68.142631
1176.976090	26.632318	68.147636
1175.520231	29.554300	68.152641
1174.818488	27.204479	68.157646
1174.207200	35.315893	68.162650
1174.038848	26.806862	68.167655
1173.700850	24.944812	68.172660
1172.714344	33.238902	68.177665
1172.209525	30.652759	68.182670
1170.873481	41.142356	68.187674
1170.062055	33.960884	68.192679
1169.978080	31.484425	68.197684
1169.473543	44.599848	68.202689
1168.542907	27.784876	68.207694
1167.438861	35.736545	68.212698
1166.901979	34.040166	68.217703
1166.712806	38.498482	68.222708
1165.642499	44.932503	68.227713
1164.985654	31.648912	68.232718
1164.427831	31.947542	68.237722
1163.749503	32.009874	68.242727
1164.017676	25.856752	68.247732
1162.481488	31.708858	68.252737
1162.417125	29.890019	68.257742
1160.962323	34.541747	68.262746
1159.904654	31.190412	68.267751
1159.457118	35.461163	68.272756
1159.187356	38.096737	68.277761
1158.906012	32.253362	68.282766
1158.336934	37.868076	68.287770
1157.582877	28.155957	68.292775
1157.035046	34.429606	68.297780
1155.635707	36.312868	68.302785
1154.758731	33.771728	68.307790
1154.084359	39.687040	68.312794
1153.821088	34.362758	68.317799
1153.489056	32.212758	68.322804
1152.678051	40.660293	68.327809
1152.766799	23.134424	68.332814
1151.421379	28.284416	68.337818
1150.982016	32.605907	68.342823
1150.114178	25.559574	68.347828
1149.101160	38.337979	68.352833
1148.603640	29.162221	68.357838
1148.088351	40.095288	68.362842
1147.243120	31.665534	68.367847
1146.594640	27.530038	68.372852
1145.911027	28.298107	68.377857
1145.699786	25.338850	68.382862
1144.700295	34.401407	68.387866
1143.559111	34.467979	68.392871
1143.383078	31.458966	68.397876
1142.363420	35.161558	68.402881
1142.181240	37.751664	68.407886
1141.170917	30.422069	68.412890
1140.766125	36.941050	68.417895
1140.348939	30.639895	68.422900
1139.592002	35.355674	68.427905
1138.708248	30.227859	68.432910
1138.042009	38.190326	68.437914
1137.417416	30.148102	68.442919
1136.782303	30.615149	68.447924
1135.408262	36.613368	68.452929
1134.875062	30.146165	68.457934
1134.652581	34.329083	68.462938
1134.295109	28.661824	68.467943
1134.152087	28.320476	68.472948
1132.845719	30.960086	68.477953
1132.201645	22.730157	68.482958
1131.724821	32.477552	68.487962
1130.920716	39.957329	68.492967
1130.123679	29.919322	68.497972
1129.170285	31.886205	68.502977
1129.190404	21.667763	68.507982
1128.103190	38.050244	68.512986
1127.270596	29.247908	68.517991
1126.752406	27.968033	68.522996
1126.174913	44.054979	68.528001
1126.076374	20.935534	68.533006
1125.123933	30.175113	68.538010
1124.196184	38.563953	68.543015
1123.761027	32.927975	68.548020
1122.450289	33.663340	68.553025
1121.958583	26.978233	68.558030
1121.560301	36.109169	68.563034
1121.043697	36.175749	68.568039
1120.666259	36.032537	68.573044
1119.541931	41.838082	68.578049
1119.235402	30.291770	68.583054
1118.374526	35.924520	68.588058
1117.419608	46.517520	68.593063
1116.971290	36.693702	68.598068
1115.989930	39.661666	68.603073
1115.689583	34.868408	68.608078
1114.863310	39.525838	68.613082
1113.915442	35.756514	68.618087
1113.501655	43.014939	68.623092
1112.697040	34.701739	68.628097
1112.702406	30.727171	68.633102
1111.888369	37.935721	68.638106
1110.589991	26.310646	68.643111
1110.538108	34.118621	68.648116
1109.627766	36.725209	68.653121
1109.739744	25.473452	68.658126
1108.324221	34.640045	68.663130
1108.030721	38.701799	68.668135
1107.227198	31.880215	68.673140
1105.897025	40.000340	68.678145
1105.588349	34.232283	68.683150
1105.056949	38.842810	68.688154
1104.594365	33.349969	68.693159
1103.530060	34.516073	68.698164
1102.442665	39.087311	68.703169
1102.469096	34.789273	68.708174
1101.916946	46.079870	68.713178
1101.513584	37.597189	68.718183
1100.566977	28.341497	68.723188
1099.647371	38.271295	68.728193
1099.530260	30.936827	68.733198
1098.424932	29.277274	68.738202
1097.697424	25.059748	68.743207
1096.915583	33.174649	68.748212
1096.289541	33.808995	68.753217
1095.954556	32.627715	68.758222
1094.768952	31.854558	68.763226
1094.229330	35.977542	68.768231
1093.959979	33.847542	68.773236
1093.501646	38.075865	68.778241
1092.690589	27.313137	68.783246
1091.401566	25.947735	68.788250
1091.284735	32.446141	68.793255
1090.971542	36.668722	68.798260
1089.840702	42.798587	68.803265
1089.400426	36.411229	68.808270
1088.765466	35.744443	68.813274
1088.029216	34.321070	68.818279
1087.039903	31.689017	68.823284
1086.344592	41.338715	68.828289
1086.071269	32.862162	68.833294
1085.560790	33.761976	68.838298
1084.930955	34.646085	68.843303
1084.259051	40.434864	68.848308
1082.948772	40.425861	68.853313
1082.127606	33.307474	68.858318
1081.343905	40.038125	68.863322
1081.107982	39.325208	68.868327
1081.136845	30.717008	68.873332
1080.393461	38.306984	68.878337
1079.518859	32.897041	68.883342
1078.822194	43.417427	68.888346
1078.220885	38.288856	68.893351
1077.196911	31.920243	68.898356
1076.413309	37.923908	68.903361
1076.215844	30.359378	68.908366
1075.441762	37.432272	68.913370
1074.150855	41.643238	68.918375
1073.597911	37.584026	68.923380
1073.212180	42.772199	68.928385
1073.296808	43.189417	68.933390
1072.232492	32.353443	68.938394
1071.496214	26.771691	68.943399
1070.937584	37.538195	68.948404
1069.912933	35.375391	68.953409
1069.259645	40.317548	68.958414
1068.604403	33.983318	68.963418
1068.188605	38.299494	68.968423
1067.995306	30.633379	68.973428
1066.891999	35.587203	68.978433
1066.232384	38.371536	68.983438
1065.610915	32.287399	68.988442
1064.354688	32.397539	68.993447
1063.811130	35.854108	68.998452
1062.909161	36.770477	69.003457
1062.750285	38.270368	69.008462
1062.243697	32.166378	69.013466
1061.606336	30.372470	69.018471
1060.748585	38.627190	69.023476
1059.984674	31.039238	69.028481
1059.887068	30.124548	69.033486
1058.837792	34.434273	69.038490
1057.794888	29.719737	69.043495
1057.250049	37.013205	69.048500
1056.719421	47.549761	69.053505
1056.793453	33.662662	69.058510
1055.628467	36.219893	69.063514
1055.100563	27.775967	69.068519
1054.520940	33.294603	69.073524
1053.168719	46.486547	69.078529
1052.621215	38.649701	69.083534
1052.163691	32.572601	69.088538
1051.631351	38.919496	69.093543
1051.612473	39.477758	69.098548
1050.274273	38.900785	69.103553
1049.431308	29.193392	69.108558
1048.805724	30.079987	69.113562
1048.108812	33.158837	69.118567
1047.450983	38.327223	69.123572
1046.746240	35.323487	69.128577
1046.534440	34.065846	69.133582
1045.662694	40.755320	69.138586
1044.600175	38.669513	69.143591
1044.156542	35.734623	69.148596
1043.848677	35.761701	69.153601
1043.404080	23.146139	69.158606
1042.427928	30.782613	69.163610
1041.650671	38.619258	69.168615
1041.528943	29.069933	69.173620
1039.986689	39.370042	69.178625
1039.469941	25.259980	69.183630
1038.931860	38.522665	69.188634
1038.596794	29.628597	69.193639
1037.944307	24.915035	69.198644
1036.905571	37.036822	69.203649
1036.797744	35.533984	69.208654
1035.815541	36.311741	69.213658
1034.453814	36.323565	69.218663
1033.725541	33.161152	69.223668
1032.921201	35.670476	69.228673
1033.118273	29.754162	69.233678
1032.641597	48.460143	69.238682
1032.450374	38.966024	69.243687
1031.800799	36.696254	69.248692
1030.778494	45.043397	69.253697
1029.816605	33.062060	69.258702
1028.810743	35.092520	69.263706
1028.215403	41.066246	69.268711
1028.109148	34.715646	69.273716
1026.707526	37.092922	69.278721
1026.254319	25.844361	69.283726
1025.699575	37.190564	69.288730
1024.958648	32.841155	69.293735
1024.944621	29.770110	69.298740
1023.955518	39.274173	69.303745
1023.334245	33.806601	69.308750
1022.394037	36.107312	69.313754
1021.955658	30.892914	69.318759
1021.217481	21.790181	69.323764
1020.148639	40.714945	69.328769
1020.008775	37.007913	69.333774
1019.184695	36.737085	69.338778
1018.265047	41.978673	69.343783
1018.063979	33.194173	69.348788
1017.246334	38.047374	69.353793
1016.889932	34.942493	69.358798
1015.898072	36.948653	69.363802
1015.159595	41.350870	69.368807
1014.850741	37.404222	69.373812
1014.171114	29.410221	69.378817
1013.364277	31.543059	69.383822
1012.135966	29.081528	69.388826
1011.645411	34.257998	69.393831
1011.667038	31.644900	69.398836
1010.377615	36.371317	69.403841
1009.574469	39.755660	69.408846
1009.304955	42.459016	69.413850
1009.071283	35.428530	69.418855
1007.995453	39.083339	69.423860
1007.006631	42.774767	69.428865
1006.505215	34.720872	69.433870
1006.320136	41.974454	69.438874
1005.679541	40.523270	69.443879
1004.806211	40.720749	69.448884
1003.974537	37.857070	69.453889
1003.442328	30.049349	69.458894
1002.144253	39.337653	69.463898
1001.460127	40.733465	69.468903
1001.409199	34.771453	69.473908
1000.726109	48.222802	69.478913
1000.658776	38.024585	69.483918
1000.065669	36.466500	69.488922
999.235760	48.302770	69.493927
997.799898	40.487442	69.498932
997.007228	43.584696	69.503937
996.732312	37.797094	69.508942
996.419672	39.031297	69.513946
995.034871	41.790687	69.518951
994.710367	33.153564	69.523956
993.941062	44.822495	69.528961
993.797835	42.538399	69.533966
992.858132	41.286197	69.538970
991.473797	34.109223	69.543975
991.466151	31.280012	69.548980
990.731610	34.249747	69.553985
990.489623	34.916049	69.558990
989.748427	36.216865	69.563994
988.525372	36.635576	69.568999
988.208302	40.276893	69.574004
987.779575	46.602582	69.579009
987.114757	39.278005	69.584014
985.820296	38.370835	69.589018
985.437620	37.444738	69.594023
985.244499	34.643462	69.599028
983.857991	38.303561	69.604033
983.448946	31.539104	69.609038
983.096498	31.242127	69.614042
982.196738	33.329837	69.619047
981.444393	27.454209	69.624052
980.742976	31.068374	69.629057
980.503489	24.259595	69.634062
979.878308	34.295534	69.639066
978.804403	36.000952	69.644071
978.488606	25.988938	69.649076
977.702983	32.812955	69.654081
976.734455	28.985477	69.659086
975.931784	37.518456	69.664090
975.503572	35.074707	69.669095
975.072179	33.740053	69.674100
974.149236	38.233132	69.679105
973.562256	32.517270	69.684110
972.626586	38.362234	69.689114
972.477008	34.595252	69.694119
972.074354	36.766290	69.699124
970.697342	39.855610	69.704129
970.243954	34.118490	69.709134
969.787830	35.623107	69.714138
969.120546	33.406635	69.719143
968.210880	30.221069	69.724148
967.546318	29.461255	69.729153
967.123091	26.313403	69.734158
966.637511	28.526020	69.739162
965.486735	41.037816	69.744167
964.763607	31.875934	69.749172
964.132491	35.543571	69.754177
963.800414	34.161576	69.759182
963.365016	34.618963	69.764186
962.208911	33.587288	69.769191
961.857189	32.273074	69.774196
961.354997	35.549616	69.779201
960.700209	25.601011	69.784206
959.581612	35.843203	69.789210
958.907987	40.834350	69.794215
958.621335	34.383156	69.799220
957.518915	31.898466	69.804225
956.778489	28.589781	69.809230
956.146515	33.612145	69.814234
955.518335	29.796747	69.819239
955.496097	26.804282	69.824244
954.877788	34.644035	69.829249
953.872766	29.428362	69.834254
952.943921	38.749393	69.839258
953.056463	27.700982	69.844263
951.937725	32.062799	69.849268
951.194088	38.616795	69.854273
950.819267	29.648649	69.859278
949.653128	30.367400	69.864282
948.629589	32.228816	69.869287
948.419932	31.048114	69.874292
947.760219	41.032788	69.879297
947.568185	25.527535	69.884302
946.550619	31.355575	69.889306
945.965485	29.830928	69.894311
945.730531	31.716664	69.899316
944.340176	33.767341	69.904321
943.391570	25.483437	69.909326
943.110861	32.971427	69.914330
942.625253	25.457506	69.919335
942.402227	21.653334	69.924340
941.220225	27.335655	69.929345
940.842404	29.143202	69.934350
940.051875	32.588633	69.939354
939.415385	27.864671	69.944359
938.520462	29.248312	69.949364
937.725792	31.563738	69.954369
937.361890	32.713065	69.959374
937.090807	34.916785	69.964378
935.772839	29.509650	69.969383
935.531812	23.918519	69.974388
934.651883	36.032408	69.979393
933.915317	24.589275	69.984398
933.020716	32.963428	69.989402
932.683186	26.965034	69.994407
932.137075	22.706082	69.999412
931.301102	38.782127	70.004417
930.755391	31.449657	70.009422
929.880919	38.432906	70.014426
929.421699	41.120725	70.019431
929.089177	31.880927	70.024436
927.583530	33.170953	70.029441
927.055960	30.545910	70.034446
926.502266	27.291096	70.039450
926.211238	24.483332	70.044455
925.735815	23.281850	70.049460
924.666415	29.941306	70.054465
924.136974	25.217660	70.059470
923.728600	27.608807	70.064474
922.577713	35.883402	70.069479
922.011611	30.424429	70.074484
921.458186	30.506371	70.079489
921.155624	38.384191	70.084494
919.914178	31.717529	70.089498
919.214100	36.873740	70.094503
918.972553	28.403206	70.099508
918.205649	36.455847	70.104513
917.948963	32.368452	70.109518
916.979414	28.257314	70.114522
916.132979	32.485924	70.119527
915.471612	37.169203	70.124532
914.799921	33.989939	70.129537
914.196866	31.369027	70.134542
913.901097	32.072280	70.139546
912.881936	31.416222	70.144551
912.258386	29.549195	70.149556
911.413367	37.863426	70.154561
911.154695	23.813263	70.159566
909.787768	28.634060	70.164570
908.855014	30.720738	70.169575
908.961992	29.907536	70.174580
908.217794	30.240613	70.179585
907.856631	27.978595	70.184590
907.157971	27.367726	70.189594
906.413114	31.808828	70.194599
906.135637	25.234764	70.199604
904.546059	32.838022	70.204609
904.292404	25.433851	70.209614
903.441916	30.973543	70.214618
903.127851	28.505336	70.219623
902.698273	22.294521	70.224628
901.561179	27.256937	70.229633
901.284733	23.466002	70.234638
900.134762	33.112392	70.239642
899.096432	36.297655	70.244647
898.720990	21.687347	70.249652
898.084903	33.347699	70.254657
898.050496	26.540987	70.259662
897.617949	26.089615	70.264666
896.734821	29.191830	70.269671
895.745209	26.019018	70.274676
894.463977	35.452916	70.279681
893.838910	28.590400	70.284686
893.392653	32.849943	70.289690
892.898618	24.766527	70.294695
892.431487	25.404015	70.299700
892.130626	26.472353	70.304705
891.496560	28.312804	70.309710
890.804070	27.139569	70.314714
889.754635	23.135774	70.319719
888.785854	31.154317	70.324724
888.106235	24.108101	70.329729
887.897539	30.892355	70.334734
887.468791	24.733450	70.339738
886.634803	26.460644	70.344743
886.340107	27.483846	70.349748
884.890600	21.738138	70.354753
884.129357	23.357561	70.359758
883.297079	39.223293	70.364762
882.861845	26.834944	70.369767
882.474621	29.527079	70.374772
881.859863	33.103821	70.379777
881.733552	18.359254	70.384782
880.435230	27.910989	70.389786
879.727696	30.445950	70.394791
879.203370	19.476838	70.399796
878.500542	34.061992	70.404801
877.495738	24.424591	70.409806
877.078496	22.527892	70.414810
876.611286	28.933826	70.419815
876.559503	26.818111	70.424820
875.207464	25.068619	70.429825
874.446737	24.133328	70.434830
874.051523	27.217815	70.439834
873.275518	29.651714	70.444839
872.706654	21.267981	70.449844
872.016045	38.416869	70.454849
871.494343	22.279719	70.459854
870.559923	26.050841	70.464858
869.592730	34.343525	70.469863
869.597688	26.035614	70.474868
868.924989	30.913091	70.479873
867.740861	23.464640	70.484878
867.272282	30.755454	70.489882
866.527832	34.289765	70.494887
866.048901	22.023496	70.499892
864.860971	25.319312	70.504897
864.571299	21.275025	70.509902
864.134164	26.081891	70.514906
863.592707	31.268059	70.519911
862.535628	22.468456	70.524916
861.872548	36.940057	70.529921
861.420603	26.479814	70.534926
860.857870	36.709256	70.539930
859.678395	28.499983	70.544935
859.245750	20.961888	70.549940
858.467133	26.862309	70.554945
858.124988	27.522487	70.559950
857.833986	26.752129	70.564954
856.905438	19.294545	70.569959
856.402447	18.182620	70.574964
855.428121	25.068236	70.579969
854.474706	16.975954	70.584974
853.798089	24.192648	70.589978
853.353607	26.580091	70.594983
853.466789	16.301138	70.599988
851.929639	22.068408	70.604993
851.209919	22.886456	70.609998
850.774600	24.387780	70.615002
850.179842	25.701595	70.620007
849.480828	17.420590	70.625012
848.535639	19.805730	70.630017
848.193006	22.479732	70.635022
848.090752	18.328347	70.640026
846.819448	32.562447	70.645031
846.192580	26.908167	70.650036
845.466681	26.623346	70.655041
844.878835	24.919387	70.660046
844.120998	23.572065	70.665050
843.345846	24.971366	70.670055
843.081214	21.393023	70.675060
841.579660	29.668269	70.680065
841.440604	21.928906	70.685070
840.967058	21.425725	70.690074
840.041641	18.055065	70.695079
839.872454	14.548263	70.700084
838.900215	20.304466	70.705089
838.227144	17.319412	70.710094
837.581131	24.039235	70.715098
836.944000	23.489554	70.720103
836.328866	6.925765	70.725108
835.330178	23.737329	70.730113
835.173509	21.056424	70.735118
834.800847	21.055996	70.740122
833.365285	28.401389	70.745127
832.834539	19.396598	70.750132
832.467384	30.228835	70.755137
831.781188	20.594361	70.760142
830.897964	31.904556	70.765146
830.244213	23.200039	70.770151
829.963681	14.693158	70.775156
828.689884	34.815934	70.780161
828.636422	27.236408	70.785166
828.015928	20.707500	70.790170
826.683075	27.711698	70.795175
826.097952	15.825046	70.800180
825.182032	24.183692	70.805185
824.737937	13.143485	70.810190
824.745702	22.838991	70.815194
823.871494	29.213524	70.820199
823.386142	25.053737	70.825204
822.305097	28.315212	70.830209
821.686831	25.253629	70.835214
821.125181	21.107565	70.840218
820.180593	22.880770	70.845223
819.731430	21.399166	70.850228
819.137630	26.413900	70.855233
818.799348	20.134958	70.860238
817.665392	24.494518	70.865242
816.859463	28.863363	70.870247
816.691424	24.279332	70.875252
815.275679	30.941922	70.880257
814.941343	14.989439	70.885262
814.220077	19.064111	70.890266
813.910518	25.536417	70.895271
813.567455	21.576330	70.900276
812.197590	30.477171	70.905281
811.917077	24.472881	70.910286
810.946131	23.627843	70.915290
810.559402	17.843889	70.920295
810.376314	21.238387	70.925300
809.341068	35.004422	70.930305
808.656777	22.662054	70.935310
807.336545	23.192514	70.940314
806.435302	31.138830	70.945319
806.260200	24.914335	70.950324
805.396675	28.262614	70.955329
805.462159	23.439563	70.960334
804.996621	30.772477	70.965338
803.976489	26.644209	70.970343
803.417992	22.776765	70.975348
802.833650	26.548951	70.980353
801.996825	24.088285	70.985358
801.282392	32.131019	70.990362
800.536015	21.206742	70.995367
800.335637	22.385248	71.000372
799.058819	34.521346	71.005377
798.704059	24.854619	71.010382
798.215936	26.884745	71.015386
797.143444	28.615243	71.020391
796.392933	20.899111	71.025396
795.662934	24.757562	71.030401
795.597158	16.079306	71.035406
794.991221	21.100706	71.040410
793.788272	23.370783	71.045415
793.357624	9.420582	71.050420
792.813946	27.667272	71.055425
792.064086	17.765409	71.060430
790.935410	17.552609	71.065434
790.447277	22.728719	71.070439
790.101610	22.187844	71.075444
789.852255	17.252492	71.080449
788.919743	14.654103	71.085454
788.416822	22.470777	71.090458
786.939759	29.162064	71.095463
786.222832	20.707315	71.100468
785.294461	23.614919	71.105473
785.489866	18.462108	71.110478
784.889750	24.001396	71.115482
784.396173	32.515169	71.120487
783.488323	20.418136	71.125492
782.351609	23.839873	71.130497
782.163775	31.393505	71.135502
781.992263	22.867696	71.140506
781.094410	25.931291	71.145511
780.477626	19.674617	71.150516
779.202309	33.526186	71.155521
778.302238	24.528168	71.160526
777.516626	27.512395	71.165530
777.154135	29.028944	71.170535
777.270115	21.219027	71.175540
776.679888	27.278708	71.180545
775.420281	19.853365	71.185550
774.677535	20.331329	71.190554
774.095264	27.331172	71.195559
773.988586	18.228927	71.200564
772.538640	29.181508	71.205569
771.769089	19.005247	71.210574
771.687583	24.911399	71.215578
770.932321	28.934727	71.220583
770.107573	22.069352	71.225588
769.312556	22.691255	71.230593
768.730174	16.301378	71.235598
768.376300	17.154243	71.240602
767.994587	17.552654	71.245607
767.410294	20.862795	71.250612
766.530735	29.105286	71.255617
765.528969	21.069626	71.260622
764.611278	17.898037	71.265626
763.851009	21.534236	71.270631
763.760366	15.337306	71.275636
762.793382	18.281026	71.280641
762.464867	17.193382	71.285646
761.873726	14.849735	71.290650
761.108111	28.462464	71.295655
760.241372	13.633962	71.300660
759.466059	17.237863	71.305665
758.956354	12.017543	71.310670
758.296621	15.377542	71.315674
757.571551	23.817783	71.320679
756.879255	15.972554	71.325684
756.199207	27.884343	71.330689
755.997138	18.131821	71.335694
754.987275	29.899005	71.340698
754.169350	23.967672	71.345703
753.671219	17.305768	71.350708
753.020673	26.557306	71.355713
752.457374	17.928303	71.360718
751.619519	23.680487	71.365722
750.688011	32.317602	71.370727
750.509795	27.216388	71.375732
750.043151	39.597253	71.380737
749.473530	25.736985	71.385742
748.519217	23.228813	71.390746
747.704744	26.335914	71.395751
746.815996	31.392892	71.400756
746.338076	31.839739	71.405761
746.093108	27.794659	71.410766
745.086659	34.500928	71.415770
744.372905	27.136924	71.420775
743.508371	27.667403	71.425780
743.127353	32.061656	71.430785
742.756367	26.197937	71.435790
741.536703	23.604285	71.440794
740.843381	35.973929	71.445799
740.587775	15.935714	71.450804
739.967189	31.785102	71.455809
739.442306	23.725565	71.460814
738.676212	33.929051	71.465818
737.851677	28.277891	71.470823
737.355877	21.265540	71.475828
736.092653	27.907037	71.480833
735.829808	27.501214	71.485838
735.190431	34.167964	71.490842
734.677869	31.562655	71.495847
734.433471	26.688020	71.500852
732.925528	37.192549	71.505857
732.642446	25.448642	71.510862
732.310828	18.053766	71.515866
730.876814	26.543814	71.520871
730.474748	19.637966	71.525876
729.562131	25.200212	71.530881
729.487780	20.919816	71.535886
728.721180	27.650975	71.540890
727.774265	28.364885	71.545895
727.443893	15.393779	71.550900
726.737269	22.697275	71.555905
725.489624	18.239422	71.560910
725.082440	25.290241	71.565914
724.327395	21.965040	71.570919
724.470382	20.736096	71.575924
722.981217	31.373252	71.580929
722.603057	16.697206	71.585934
722.103536	22.821298	71.590938
721.645774	16.331169	71.595943
720.694521	18.750435	71.600948
719.716121	21.541450	71.605953
719.555730	26.559732	71.610958
719.029526	26.183229	71.615962
717.915745	22.855225	71.620967
717.286809	20.006681	71.625972
716.476556	25.035398	71.630977
716.255802	20.213773	71.635982
714.997679	31.779228	71.640986
714.264590	37.275051	71.645991
714.160614	24.772511	71.650996
713.792778	29.084244	71.656001
712.959763	26.627735	71.661006
712.174672	23.220590	71.666010
711.302772	24.103908	71.671015
710.967600	27.115778	71.676020
709.653926	32.741893	71.681025
709.042421	20.837404	71.686030
708.520571	21.336984	71.691034
708.325587	21.962710	71.696039
707.852330	18.020220	71.701044
706.808276	25.306488	71.706049
706.350599	24.944307	71.711054
705.343033	23.906449	71.716058
704.911483	28.434906	71.721063
704.338196	21.658826	71.726068
703.804064	28.441284	71.731073
703.032878	17.634540	71.736078
702.056683	17.279231	71.741082
701.617923	25.336432	71.746087
701.171996	19.549311	71.751092
700.227583	20.470988	71.756097
699.122999	21.973249	71.761102
698.644599	22.166295	71.766106
698.201366	25.900261	71.771111
697.631627	23.673068	71.776116
696.434279	28.646738	71.781121
696.338337	12.640565	71.786126
695.604195	18.650633	71.791130
694.889367	21.342917	71.796135
694.430859	14.889185	71.801140
693.366583	23.326682	71.806145
692.880936	20.944176	71.811150
692.588904	22.891057	71.816154
691.719582	26.237140	71.821159
691.007786	14.484249	71.826164
690.686358	32.569402	71.831169
689.440445	17.345576	71.836174
688.562946	28.170772	71.841178
687.858646	32.260123	71.846183
687.718572	12.727073	71.851188
687.188551	20.790920	71.856193
686.336744	24.824911	71.861198
685.358511	27.738913	71.866202
684.731022	29.105286	71.871207
684.667419	20.929736	71.876212
683.900960	31.536984	71.881217
682.908887	18.393715	71.886222
682.372456	21.377712	71.891226
681.776260	28.460211	71.896231
681.033754	23.795789	71.901236
680.146111	21.664955	71.906241
679.733259	26.392284	71.911246
679.352119	23.830715	71.916250
678.281100	27.844424	71.921255
677.838876	17.800581	71.926260
677.055470	28.205525	71.931265
676.198405	23.010574	71.936270
675.463671	17.731492	71.941274
674.606809	24.596883	71.946279
674.555296	11.696504	71.951284
673.825321	28.862705	71.956289
673.450705	23.851123	71.961294
672.258450	20.198175	71.966298
671.508714	26.567121	71.971303
671.571522	20.768380	71.976308
670.449875	26.248815	71.981313
669.730941	21.777760	71.986318
669.372467	21.967484	71.991322
668.652309	28.003719	71.996327
667.803440	17.882711	72.001332
666.973433	18.710488	72.006337
666.384409	16.264028	72.011342
666.140826	18.988507	72.016346
665.317577	24.411964	72.021351
664.647303	16.646838	72.026356
664.085420	18.786502	72.031361
663.425304	20.339422	72.036366
662.628403	19.209689	72.041370
661.804589	24.286311	72.046375
661.723932	18.505687	72.051380
660.455654	22.758969	72.056385
659.752753	24.949476	72.061390
659.038544	12.170402	72.066394
658.653395	23.182120	72.071399
657.851163	15.354434	72.076404
657.046349	17.619517	72.081409
656.525931	19.959158	72.086414
656.175925	14.779663	72.091418
655.231971	24.125247	72.096423
654.788279	15.187075	72.101428
653.875791	17.622268	72.106433
653.253488	24.936006	72.111438
652.417477	18.942940	72.116442
651.553152	20.047420	72.121447
651.257283	15.595731	72.126452
650.684781	25.265357	72.131457
650.036106	25.635337	72.136462
649.469714	16.175819	72.141466
648.357849	30.573828	72.146471
647.935527	23.866762	72.151476
647.671396	25.670434	72.156481
646.881069	23.363267	72.161486
645.770603	30.734251	72.166490
645.373015	23.606937	72.171495
644.966223	26.721681	72.176500
643.441931	27.694726	72.181505
643.319421	18.669137	72.186510
642.775201	31.223201	72.191514
642.549956	23.513361	72.196519
641.659067	22.982067	72.201524
640.784000	30.589949	72.206529
640.189624	26.548492	72.211534
639.621483	21.036312	72.216538
638.526292	26.343814	72.221543
638.299094	25.309437	72.226548
637.347930	29.717231	72.231553
636.750629	26.426860	72.236558
635.923198	28.578859	72.241562
635.089450	27.964351	72.246567
634.793009	18.261574	72.251572
634.330721	24.020209	72.256577
633.842346	27.329295	72.261582
632.664305	21.192014	72.266586
632.371641	24.294892	72.271591
631.426680	16.896795	72.276596
630.672122	28.445159	72.281601
630.249069	24.165111	72.286606
629.755701	30.122661	72.291610
628.778613	31.923188	72.296615
628.235540	18.134439	72.301620
627.201120	32.742469	72.306625
626.975949	24.961657	72.311630
626.081894	19.506118	72.316634
625.295104	29.317109	72.321639
625.019812	27.110848	72.326644
624.303450	21.581278	72.331649
623.959352	19.925287	72.336654
622.908293	32.632613	72.341658
622.338952	25.346580	72.346663
621.860367	18.826676	72.351668
620.660849	34.277853	72.356673
619.983544	27.630325	72.361678
619.730934	23.171750	72.366682
619.221429	32.650004	72.371687
618.316177	17.078663	72.376692
617.447852	34.451410	72.381697
616.824308	26.615777	72.386702
616.669231	29.936437	72.391706
615.617545	36.273067	72.396711
614.976960	17.234479	72.401716
614.181750	28.789321	72.406721
613.770612	33.694580	72.411726
613.007189	23.022251	72.416730
612.063624	33.468489	72.421735
611.604198	20.196271	72.426740
611.017106	22.597001	72.431745
610.507856	26.801958	72.436750
609.618752	25.120808	72.441754
608.958665	28.268014	72.446759
608.702471	15.693552	72.451764
607.694809	39.361526	72.456769
606.825319	31.443641	72.461774
606.222711	33.931999	72.466778
605.907042	31.241745	72.471783
605.344296	19.010991	72.476788
604.261843	30.127467	72.481793
604.053361	16.870479	72.486798
603.255647	34.787062	72.491802
602.233252	31.463481	72.496807
601.692901	28.528320	72.501812
601.295933	31.769238	72.506817
600.580621	23.606033	72.511822
599.431613	20.827739	72.516826
599.259101	29.612087	72.521831
598.735830	23.033074	72.526836
597.830564	23.740398	72.531841
596.827905	22.668689	72.536846
596.381310	17.190780	72.541850
595.552066	34.809615	72.546855
595.388003	18.456345	72.551860
594.779616	31.011171	72.556865
593.628934	32.077702	72.561870
593.257699	30.925924	72.566874
592.613755	29.484849	72.571879
591.847828	25.259421	72.576884
590.940919	22.355839	72.581889
590.590891	24.876508	72.586894
590.033705	37.647110	72.591898
589.051624	32.637681	72.596903
588.420831	19.939960	72.601908
587.781130	24.447969	72.606913
587.646447	22.839051	72.611918
586.785170	21.189747	72.616922
585.869953	25.987641	72.621927
585.531863	30.188995	72.626932
584.463308	30.360945	72.631937
583.732488	28.553670	72.636942
583.052556	21.233227	72.641946
582.554391	34.719813	72.646951
582.761716	25.881386	72.651956
581.446515	30.771376	72.656961
580.830172	29.559294	72.661966
580.370201	25.915909	72.666970
579.133088	22.366347	72.671975
579.032639	26.906735	72.676980
578.082249	25.837746	72.681985
576.882691	25.891796	72.686990
576.220955	34.249452	72.691994
575.525425	28.405923	72.696999
575.213763	24.691610	72.702004
574.813505	26.865472	72.707009
574.317954	29.032437	72.712014
573.999558	21.949296	72.717018
572.753246	25.022731	72.722023
572.359337	23.757876	72.727028
571.278024	26.142720	72.732033
570.692328	31.630867	72.737038
570.239736	25.499490	72.742042
568.951268	27.092597	72.747047
568.229612	22.634625	72.752052
567.404636	29.108620	72.757057
567.281919	29.145690	72.762062
567.243840	29.285971	72.767066
566.461637	31.430788	72.772071
565.914814	27.413316	72.777076
564.521124	36.710723	72.782081
564.501893	29.272426	72.787086
563.342767	27.482919	72.792090
562.252593	31.062915	72.797095
562.324317	17.852765	72.802100
562.013435	24.109255	72.807105
560.609918	21.209096	72.812110
559.984074	23.431509	72.817114
559.198979	25.086363	72.822119
559.209802	21.472070	72.827124
558.291319	20.396430	72.832129
557.633011	19.995273	72.837134
557.126944	20.916564	72.842138
556.248503	19.656353	72.847143
555.462604	18.860788	72.852148
554.588109	20.277576	72.857153
554.214126	24.686495	72.862158
553.860147	17.298374	72.867162
552.458443	17.950753	72.872167
552.070159	10.722640	72.877172
551.545774	25.856555	72.882177
551.227071	14.386454	72.887182
550.361914	16.501911	72.892186
549.480389	15.046656	72.897191
549.168239	10.930311	72.902196
548.401657	14.244301	72.907201
547.736151	26.057608	72.912206
547.273222	19.666116	72.917210
546.379880	22.572952	72.922215
545.036303	11.770728	72.927220
544.227118	16.744127	72.932225
543.696414	18.055692	72.937230
543.840225	15.292258	72.942234
543.105720	15.702746	72.947239
542.994732	16.509066	72.952244
541.777027	24.792862	72.957249
540.886209	20.230962	72.962254
540.554062	25.468991	72.967258
539.358804	20.749010	72.972263
538.924446	24.166199	72.977268
538.033266	21.414672	72.982273
537.527066	26.350849	72.987278
537.586989	16.198673	72.992282
536.528414	25.269241	72.997287
535.974943	16.706552	73.002292
535.336772	25.442073	73.007297
534.250733	20.632158	73.012302
533.436949	15.400412	73.017306
532.962958	24.611242	73.022311
532.848523	22.016676	73.027316
531.457134	19.709106	73.032321
530.701090	15.846399	73.037326
530.876023	26.360477	73.042330
530.144988	25.321218	73.047335
529.269718	13.356321	73.052340
528.282545	24.140676	73.057345
527.790476	22.525617	73.062350
527.060185	19.152387	73.067354
526.006764	20.539340	73.072359
525.940658	27.384458	73.077364
524.971212	29.852424	73.082369
524.549774	26.100414	73.087374
524.134349	23.109103	73.092378
523.378905	19.631072	73.097383
522.722044	24.700060	73.102388
521.761005	19.398736	73.107393
520.911937	25.799310	73.112398
520.231475	24.701536	73.117402
519.593576	35.603723	73.122407
519.402362	24.764585	73.127412
518.917408	29.689497	73.132417
518.000234	17.180929	73.137422
517.260145	26.265422	73.142426
516.719074	23.707284	73.147431
515.867903	17.305111	73.152436
515.113688	23.140227	73.157441
514.638632	19.259569	73.162446
514.052917	22.681949	73.167450
513.066807	23.389568	73.172455
512.842151	18.825633	73.177460
511.983984	26.762010	73.182465
511.297249	17.968250	73.187470
510.608240	26.194642	73.192474
509.695957	26.098882	73.197479
509.480412	23.775888	73.202484
508.823331	24.345937	73.207489
507.817020	23.647001	73.212494
507.357253	13.910352	73.217498
506.507177	34.309488	73.222503
506.275938	20.001179	73.227508
504.970300	18.936775	73.232513
504.578326	26.144460	73.237518
503.979074	23.007400	73.242522
503.502679	28.616914	73.247527
502.608293	29.846080	73.252532
501.673195	27.398026	73.257537
501.122321	18.820741	73.262542
500.892555	24.498194	73.267546
500.277607	24.198953	73.272551
499.570037	10.062734	73.277556
498.691848	32.428044	73.282561
498.292555	21.152137	73.287566
497.462497	21.174168	73.292570
496.497921	17.806733	73.297575
496.029434	16.407118	73.302580
495.617989	17.387462	73.307585
494.621920	18.590252	73.312590
494.249440	22.207320	73.317594
493.656002	27.600520	73.322599
493.136322	17.444493	73.327604
492.082435	17.475377	73.332609
491.164195	15.496144	73.337614
490.748575	14.190609	73.342618
490.205957	24.006878	73.347623
489.633934	16.711856	73.352628
488.570385	27.724431	73.357633
488.010702	11.609263	73.362638
487.867744	17.758578	73.367642
486.884675	24.018086	73.372647
486.097137	18.922522	73.377652
485.772438	25.411449	73.382657
485.003239	15.973259	73.387662
484.111209	23.686382	73.392666
483.532640	22.651232	73.397671
483.236273	17.054800	73.402676
481.988176	22.875570	73.407681
481.043283	13.287181	73.412686
480.663111	18.750480	73.417690
479.946683	24.360391	73.422695
479.867552	13.976491	73.427700
479.067323	18.306671	73.432705
478.168309	23.097286	73.437710
477.874836	10.667569	73.442714
476.989706	17.865514	73.447719
476.172632	15.680938	73.452724
475.496733	24.045593	73.457729
475.189328	20.403158	73.462734
474.712925	10.147209	73.467738
473.340919	18.849844	73.472743
472.666997	23.006942	73.477748
472.188105	17.769171	73.482753
471.977158	17.203724	73.487758
471.160080	20.005395	73.492762
470.415164	19.528176	73.497767
470.010872	18.422686	73.502772
468.804492	22.879080	73.507777
467.658327	18.737933	73.512782
467.481060	14.011917	73.517786
466.946926	23.446797	73.522791
466.746721	20.183093	73.527796
465.738125	25.893173	73.532801
465.155343	11.631432	73.537806
464.610291	21.591590	73.542810
463.581467	22.214572	73.547815
462.970883	19.263829	73.552820
462.007177	19.889052	73.557825
462.026267	13.605286	73.562830
461.338292	18.179356	73.567834
459.916064	32.898102	73.572839
459.649021	21.178518	73.577844
459.247648	25.563427	73.582849
458.912401	19.772924	73.587854
457.548260	18.035057	73.592858
456.762175	23.331225	73.597863
456.704434	21.252749	73.602868
455.964427	17.158858	73.607873
455.078170	15.185583	73.612878
454.885730	14.979881	73.617882
453.952388	21.474322	73.622887
452.902066	20.269921	73.627892
452.399147	21.952386	73.632897
451.594218	5.292852	73.637902
451.547409	18.710669	73.642906
450.578280	14.113978	73.647911
449.929013	14.380027	73.652916
448.936548	26.664906	73.657921
448.817135	18.162392	73.662926
448.055330	11.408549	73.667930
446.982968	19.008490	73.672935
446.649466	22.950507	73.677940
446.381637	17.395266	73.682945
445.106693	17.560738	73.687950
444.443660	18.997485	73.692954
443.940012	18.133330	73.697959
443.395379	10.327769	73.702964
442.517915	14.884726	73.707969
442.029333	23.260541	73.712974
441.295125	14.203142	73.717978
440.331839	19.360393	73.722983
439.735282	11.345489	73.727988
439.226835	14.080646	73.732993
438.797849	12.315211	73.737998
438.236342	15.312708	73.743002
436.920091	22.703937	73.748007
436.257820	16.885124	73.753012
436.026776	16.034305	73.758017
435.371634	17.912913	73.763022
434.832409	9.363760	73.768026
433.776221	22.205986	73.773031
433.497298	7.608844	73.778036
432.936366	22.098891	73.783041
431.904889	18.480374	73.788046
431.010516	11.787083	73.793050
430.433475	11.250012	73.798055
430.622397	12.692935	73.803060
429.320234	13.644907	73.808065
428.368528	8.783681	73.813070
427.981182	3.152878	73.818074
427.811470	14.182306	73.823079
427.113846	8.988864	73.828084
426.158691	14.307246	73.833089
425.593465	13.159599	73.838094
424.786310	12.449465	73.843098
423.423344	18.089869	73.848103
423.208043	11.911263	73.853108
422.949076	11.490665	73.858113
422.453195	13.775976	73.863118
421.544165	13.359615	73.868122
420.565165	17.887028	73.873127
420.189732	15.196868	73.878132
419.834164	18.156824	73.883137
418.558187	16.573663	73.888142
418.496679	15.296868	73.893146
417.584033	17.935591	73.898151
416.688793	11.469523	73.903156
415.891046	20.006564	73.908161
415.482889	18.843353	73.913166
414.655590	21.627747	73.918170
414.382654	20.211181	73.923175
413.396118	6.652457	73.928180
412.753751	13.994658	73.933185
412.241737	18.592739	73.938190
412.058579	17.977138	73.943194
410.933133	23.858819	73.948199
410.378848	14.859492	73.953204
409.671740	16.777925	73.958209
408.752899	14.103397	73.963214
407.902392	15.136372	73.968218
407.503051	17.910919	73.973223
407.085148	5.669784	73.978228
406.349268	6.834300	73.983233
405.386804	17.289900	73.988238
404.676073	11.179206	73.993242
404.355895	9.883709	73.998247
404.126611	18.778014	74.003252
403.124956	19.614306	74.008257
402.313078	17.638660	74.013262
401.655929	15.412858	74.018266
400.608792	12.471777	74.023271
399.971643	9.534749	74.028276
399.404352	17.847415	74.033281
398.996921	20.591715	74.038286
398.929392	13.661024	74.043290
397.828282	18.580058	74.048295
397.017326	6.628637	74.053300
396.590786	16.152029	74.058305
395.170573	17.763063	74.063310
394.805966	20.962578	74.068314
394.054841	25.609806	74.073319
394.106650	15.342244	74.078324
393.419890	11.209929	74.083329
392.382956	12.627425	74.088334
391.753780	17.389256	74.093338
391.227058	22.210456	74.098343
390.597062	10.969775	74.103348
389.529699	6.762499	74.108353
388.977580	14.336323	74.113358
388.409977	14.564143	74.118362
387.521106	30.787463	74.123367
386.600657	13.528207	74.128372
385.978930	15.672733	74.133377
385.700581	25.010093	74.138382
385.511717	13.377421	74.143386
384.598980	30.052391	74.148391
383.909592	16.419514	74.153396
383.238629	27.867868	74.158401
382.863258	19.081306	74.163406
381.824012	13.035586	74.168410
380.769827	22.241119	74.173415
380.750795	9.624193	74.178420
380.095065	18.966496	74.183425
378.831559	12.619054	74.188430
378.175381	11.563182	74.193434
377.610584	13.769599	74.198439
377.770618	13.272772	74.203444
376.713181	8.970881	74.208449
375.454063	13.276448	74.213454
375.575040	11.571613	74.218458
374.566346	8.611803	74.223463
373.755218	11.923477	74.228468
373.090723	16.113786	74.233473
372.316326	16.773528	74.238478
372.308880	7.553033	74.243482
371.099632	10.297384	74.248487
370.608601	11.684661	74.253492
370.174345	9.612578	74.258497
369.722803	14.019682	74.263502
368.924011	12.240655	74.268506
368.053904	17.479272	74.273511
367.240428	13.319852	74.278516
365.951922	14.231834	74.283521
365.713138	15.438567	74.288526
365.408177	10.944223	74.293530
364.927330	17.880654	74.298535
364.394659	15.855795	74.303540
363.319501	17.618433	74.308545
362.461160	23.567950	74.313550
362.439302	2.917046	74.318554
361.188012	23.906817	74.323559
360.341484	7.048957	74.328564
359.981419	21.992690	74.333569
359.478193	27.134998	74.338574
358.407944	16.590527	74.343578
357.755854	25.511219	74.348583
357.472677	18.841975	74.353588
357.013201	30.404861	74.358593
356.120514	12.064159	74.363598
355.273387	19.574621	74.368602
354.442476	21.005030	74.373607
354.139235	13.944755	74.378612
353.637540	26.656061	74.383617
352.492296	15.229430	74.388622
352.219022	19.445703	74.393626
351.560289	26.156605	74.398631
351.037484	25.281331	74.403636
349.824101	16.101641	74.408641
349.403324	33.135025	74.413646
349.296991	13.580921	74.418650
348.402686	26.108798	74.423655
347.572274	15.759496	74.428660
346.962750	21.866477	74.433665
345.996597	23.772598	74.438670
345.428559	16.312986	74.443674
344.491934	20.313288	74.448679
344.321848	24.673964	74.453684
343.492110	23.197915	74.458689
342.483669	23.920198	74.463694
341.701948	12.539716	74.468698
341.398579	14.341783	74.473703
341.161596	15.349537	74.478708
340.736429	21.827676	74.483713
339.506078	13.860200	74.488718
339.116813	12.764954	74.493722
338.189364	14.015215	74.498727
337.154848	12.420422	74.503732
336.303219	19.542107	74.508737
335.822560	26.352362	74.513742
335.821394	13.783053	74.518746
335.323703	22.996101	74.523751
334.569524	15.529890	74.528756
333.875505	31.485627	74.533761
333.129987	24.461149	74.538766
332.669447	22.979877	74.543770
331.248034	17.584860	74.548775
331.044991	18.935707	74.553780
330.205096	25.584025	74.558785
329.562278	25.590462	74.563790
329.118546	23.297549	74.568794
328.426113	24.575011	74.573799
328.164795	21.838294	74.578804
326.933753	27.413569	74.583809
326.234783	25.061991	74.588814
326.165666	14.439978	74.593818
324.812215	20.738070	74.598823
324.133300	13.885908	74.603828
323.368946	21.933534	74.608833
323.181042	17.608192	74.613838
322.780992	19.376786	74.618842
321.434537	31.139391	74.623847
320.990475	17.070054	74.628852
320.715742	28.523073	74.633857
319.781747	25.105108	74.638862
319.030074	20.136352	74.643866
318.571721	28.964673	74.648871
318.037297	22.488442	74.653876
316.862289	17.208699	74.658881
316.284663	25.699644	74.663886
315.846658	14.797389	74.668890
315.112637	24.995840	74.673895
314.454564	19.897051	74.678900
313.567622	21.620251	74.683905
313.265099	22.236338	74.688910
312.709908	23.856200	74.693914
311.297078	27.951339	74.698919
310.728217	17.039980	74.703924
310.462968	32.629340	74.708929
310.064718	21.873707	74.713934
309.631759	25.527243	74.718938
308.395026	17.814686	74.723943
307.602872	22.548898	74.728948
307.270589	25.169271	74.733953
306.571128	27.414515	74.738958
305.797521	13.916520	74.743962
305.082724	20.935981	74.748967
304.898799	14.317160	74.753972
303.798838	21.133089	74.758977
302.692767	16.283905	74.763982
302.396129	17.875173	74.768986
301.673780	26.510611	74.773991
301.646487	26.436291	74.778996
300.398543	19.812026	74.784001
299.751094	23.359405	74.789006
299.697160	19.312328	74.794010
299.003968	21.972882	74.799015
297.949781	19.854548	74.804020
297.123846	19.215257	74.809025
296.447876	25.358071	74.814030
296.051746	25.003503	74.819034
294.740608	25.535937	74.824039
294.442671	26.659067	74.829044
294.003176	13.199284	74.834049
293.703002	26.335780	74.839054
292.965283	11.532688	74.844058
292.077712	30.435011	74.849063
291.525062	8.633990	74.854068
290.296768	25.337194	74.859073
289.484792	6.081671	74.864078
289.316231	9.467561	74.869082
288.734697	21.597093	74.874087
288.594948	15.811733	74.879092
287.513319	28.306408	74.884097
286.803561	26.606254	74.889102
286.230767	27.971889	74.894106
284.985289	37.534378	74.899111
284.283857	25.704305	74.904116
284.048927	32.376053	74.909121
283.726872	26.976134	74.914126
283.405335	20.793980	74.919130
282.078547	30.453004	74.924135
281.246374	17.248200	74.929140
280.770102	28.793267	74.934145
279.468441	27.509158	74.939150
279.132091	17.927940	74.944154
278.263408	34.211143	74.949159
278.338011	29.985883	74.954164
277.956735	20.750864	74.959169
276.850857	33.175295	74.964174
276.192698	22.339678	74.969178
275.490469	29.025991	74.974183
275.660126	18.690768	74.979188
274.052675	26.432837	74.984193
273.711933	30.915335	74.989198
272.982179	20.222018	74.994202
271.493785	24.934762	74.999207
270.854987	20.512569	75.004212
270.160775	27.408913	75.009217
270.093095	29.433611	75.014222
269.852930	24.373873	75.019226
269.288659	31.405621	75.024231
268.709766	27.350763	75.029236
268.002626	34.149825	75.034241
266.915490	26.921211	75.039246
266.156523	26.072563	75.044250
265.213624	26.879044	75.049255
265.057307	26.535138	75.054260
264.285390	26.853903	75.059265
262.965328	33.996670	75.064270
262.694412	34.918380	75.069274
262.237772	31.591497	75.074279
262.237793	38.164296	75.079284
261.244356	33.092173	75.084289
260.198417	37.401664	75.089294
259.880956	27.593511	75.094298
258.662907	42.757610	75.099303
258.050108	31.047452	75.104308
257.394989	30.522868	75.109313
257.002937	26.629038	75.114318
256.823118	29.898460	75.119322
255.666597	33.135925	75.124327
254.856442	28.684282	75.129332
254.460547	26.930951	75.134337
253.544414	35.324488	75.139342
252.905327	27.778456	75.144346
251.902522	23.464757	75.149351
251.787633	26.857867	75.154356
251.461115	25.878785	75.159361
250.889104	28.751843	75.164366
250.312951	26.823825	75.169370
248.621753	28.959103	75.174375
248.070016	26.984616	75.179380
247.241206	25.016454	75.184385
246.983523	23.171708	75.189390
246.602755	20.693737	75.194394
246.024342	30.835859	75.199399
245.352081	18.209542	75.204404
244.557484	21.058159	75.209409
243.932152	27.207104	75.214414
243.047562	18.694139	75.219418
242.382781	29.228491	75.224423
241.847701	20.522617	75.229428
241.730600	18.661768	75.234433
240.136498	26.496344	75.239438
239.798097	28.794431	75.244442
239.259244	28.282856	75.249447
238.496234	20.258280	75.254452
237.481661	26.554432	75.259457
236.821667	20.028859	75.264462
236.591565	24.435373	75.269466
236.133038	27.798111	75.274471
235.451975	19.968627	75.279476
234.352372	25.880950	75.284481
233.850867	24.209114	75.289486
233.374289	11.852804	75.294490
232.428668	18.368192	75.299495
231.706911	22.987125	75.304500
231.310635	25.609824	75.309505
230.792872	27.662121	75.314510
229.985868	24.821603	75.319514
229.044855	31.777802	75.324519
228.784294	17.114703	75.329524
228.153374	14.610385	75.334529
226.824105	21.475515	75.339534
226.317803	19.728754	75.344538
225.823826	22.699759	75.349543
225.574262	12.309953	75.354548
224.597819	16.373412	75.359553
223.782348	23.957710	75.364558
223.395045	19.173746	75.369562
222.889476	22.491946	75.374567
222.425919	15.085102	75.379572
221.227449	20.793997	75.384577
220.334845	20.963285	75.389582
220.216200	9.163341	75.394586
218.897086	17.994853	75.399591
218.759775	20.938959	75.404596
218.219354	25.394948	75.409601
217.432922	22.272040	75.414606
216.626928	18.026329	75.419610
215.672972	29.966095	75.424615
215.822995	24.651774	75.429620
215.265308	31.900096	75.434625
213.492070	32.246053	75.439630
213.372818	25.068160	75.444634
213.109742	26.572087	75.449639
212.044428	21.427872	75.454644
211.349575	29.757754	75.459649
210.617311	32.009830	75.464654
210.270973	19.369411	75.469658
209.082912	36.550354	75.474663
208.257567	19.856338	75.479668
207.840885	32.580912	75.484673
207.126327	32.647703	75.489678
207.241668	29.407835	75.494682
206.652484	26.589367	75.499687
205.949559	21.349534	75.504692
204.875350	19.923550	75.509697
203.891699	28.985438	75.514702
203.064784	20.873295	75.519706
202.226561	26.210959	75.524711
202.106936	14.691862	75.529716
201.816417	30.734666	75.534721
201.085314	32.537136	75.539726
200.502245	30.340579	75.544730
199.870471	24.412903	75.549735
198.871938	29.005011	75.554740
197.772682	38.542646	75.559745
197.099328	40.255488	75.564750
197.121781	38.679891	75.569754
196.232726	43.563627	75.574759
195.718109	37.364960	75.579764
194.279046	28.946722	75.584769
194.111121	34.011944	75.589774
193.863393	39.394237	75.594778
193.293200	30.042701	75.599783
192.282181	22.863492	75.604788
191.713050	38.986994	75.609793
191.043570	39.798796	75.614798
190.341289	33.708898	75.619802
189.346172	39.386969	75.624807
189.075743	32.416103	75.629812
188.623270	30.547227	75.634817
187.392341	29.294468	75.639822
187.013378	28.033604	75.644826
186.107074	35.774323	75.649831
185.905268	30.664327	75.654836
184.940445	34.792182	75.659841
184.154583	29.876231	75.664846
183.764156	23.851733	75.669850
183.339322	33.045301	75.674855
182.687638	35.259307	75.679860
181.522042	38.461983	75.684865
181.187211	39.267739	75.689870
180.547304	28.577475	75.694874
179.049292	35.898462	75.699879
179.020447	27.141850	75.704884
178.470382	31.687692	75.709889
177.669564	27.343398	75.714894
176.831486	25.321546	75.719898
176.301833	34.637482	75.724903
176.050119	27.651022	75.729908
175.683484	32.371041	75.734913
174.189780	29.558033	75.739918
173.955567	25.591745	75.744922
173.241879	27.079215	75.749927
172.362015	25.661681	75.754932
171.611047	29.509442	75.759937
170.517117	38.702468	75.764942
170.870027	26.122447	75.769946
169.866650	33.463917	75.774951
168.816147	29.785475	75.779956
168.362391	25.045232	75.784961
167.791269	29.573934	75.789966
167.593657	25.535580	75.794970
166.252034	32.352252	75.799975
165.625790	30.597819	75.804980
165.220502	23.798273	75.809985
164.892454	34.075526	75.814990
164.090153	25.951588	75.819994
162.757831	24.880586	75.824999
162.545547	24.629188	75.830004
162.203752	28.678209	75.835009
161.414455	25.483238	75.840014
160.680411	27.158457	75.845018
160.156393	28.033804	75.850023
159.148793	27.133373	75.855028
158.281767	29.782259	75.860033
158.284843	24.339984	75.865038
157.807684	20.664745	75.870042
155.910392	31.752022	75.875047
155.531744	21.542076	75.880052
155.130804	24.193913	75.885057
154.662160	24.858585	75.890062
154.473978	22.554922	75.895066
152.981007	23.915925	75.900071
152.768186	19.581962	75.905076
152.195175	18.462431	75.910081
150.820248	26.769879	75.915086
150.473301	23.908070	75.920090
149.887132	25.518713	75.925095
149.638714	19.766466	75.930100
149.191894	14.459010	75.935105
148.245302	24.584155	75.940110
147.628157	21.476856	75.945114
146.561427	27.890164	75.950119
145.937869	25.898770	75.955124
145.463993	34.541932	75.960129
144.666851	32.313294	75.965134
144.026296	26.565227	75.970138
142.777321	23.762101	75.975143
142.516428	17.251768	75.980148
142.002536	26.265575	75.985153
141.889164	21.352793	75.990158
140.818508	22.714270	75.995162
139.649331	26.981956	76.000167
139.550079	26.510690	76.005172
139.196193	26.827489	76.010177
137.783934	26.707516	76.015182
137.415270	14.978989	76.020186
136.632708	22.715753	76.025191
136.298729	31.014913	76.030196
135.577605	30.546618	76.035201
134.833553	25.463174	76.040206
134.455259	19.730062	76.045210
133.394083	22.810452	76.050215
132.828356	23.083763	76.055220
132.183654	24.937127	76.060225
131.477847	30.816658	76.065230
130.919124	24.180356	76.070234
129.899545	17.168123	76.075239
129.719587	28.289064	76.080244
129.039135	25.291210	76.085249
128.089019	22.524012	76.090254
127.521313	17.220068	76.095258
126.467505	26.441396	76.100263
126.347855	31.060535	76.105268
125.308947	34.940034	76.110273
124.305489	38.006495	76.115278
124.200973	27.077917	76.120282
123.759095	32.864902	76.125287
123.453594	28.812219	76.130292
122.352589	24.727124	76.135297
121.511443	25.425972	76.140302
121.160422	21.476743	76.145306
120.240968	28.913651	76.150311
119.489167	23.402526	76.155316
118.900827	19.902719	76.160321
118.392884	22.500662	76.165326
117.857823	32.984388	76.170330
116.817893	29.903516	76.175335
116.652607	24.969053	76.180340
115.862645	30.573431	76.185345
114.829401	28.454993	76.190350
114.568799	21.589810	76.195354
113.504306	32.397656	76.200359
112.829550	17.207717	76.205364
112.276243	29.542502	76.210369
111.414174	22.686503	76.215374
111.462555	7.633564	76.220378
110.325431	28.909551	76.225383
109.512399	16.644778	76.230388
109.148095	21.801237	76.235393
108.386676	28.500178	76.240398
108.245571	20.149403	76.245402
106.929588	29.612817	76.250407
106.502903	28.454193	76.255412
105.939245	29.457295	76.260417
104.722462	22.697289	76.265422
104.141799	23.652642	76.270426
103.427553	24.097874	76.275431
103.051352	20.250434	76.280436
102.237776	22.405121	76.285441
101.184782	34.387522	76.290446
100.895318	24.562328	76.295450
99.982855	30.228822	76.300455
99.997942	26.265365	76.305460
99.449463	26.446048	76.310465
98.818135	30.418249	76.315470
98.011811	17.936373	76.320474
97.222572	27.533403	76.325479
96.640544	13.391533	76.330484
95.893550	22.937669	76.335489
95.014760	29.283179	76.340494
94.831116	22.694302	76.345498
93.592560	30.634685	76.350503
93.210871	26.537389	76.355508
92.796300	19.387689	76.360513
91.977430	25.971218	76.365518
91.108719	26.922049	76.370522
90.080118	32.819954	76.375527
89.891692	21.190421	76.380532
89.668277	19.537346	76.385537
88.565272	28.749187	76.390542
88.128720	18.037574	76.395546
87.125769	29.371765	76.400551
86.515228	30.218348	76.405556
85.430415	32.808952	76.410561
84.777030	26.036375	76.415566
84.592493	34.347975	76.420570
83.996833	29.879536	76.425575
83.725440	32.080224	76.430580
82.824939	33.327859	76.435585
81.792890	34.710012	76.440590
81.819489	23.137649	76.445594
80.183579	29.607063	76.450599
79.653682	21.433413	76.455604
79.149493	24.721456	76.460609
78.607436	33.747650	76.465614
78.477334	24.759623	76.470618
77.468579	29.014367	76.475623
76.560718	25.494567	76.480628
76.397128	26.675140	76.485633
75.110289	31.805273	76.490638
74.722742	23.142151	76.495642
74.036772	30.166530	76.500647
73.432572	31.333797	76.505652
72.428655	35.695004	76.510657
71.559845	30.844362	76.515662
71.765755	26.673857	76.520666
71.103986	32.708802	76.525671
70.110333	36.298835	76.530676
69.133827	32.359485	76.535681
68.665692	29.029749	76.540686
68.437094	29.138923	76.545690
67.135322	33.653289	76.550695
66.577365	28.732572	76.555700
66.172467	30.415247	76.560705
65.652247	40.858771	76.565710
65.043656	30.296017	76.570714
64.088069	40.206593	76.575719
63.651773	28.003171	76.580724
62.814650	31.781125	76.585729
61.505703	36.187831	76.590734
61.166650	31.560203	76.595738
60.756248	26.854070	76.600743
60.591986	30.311826	76.605748
59.847951	22.159718	76.610753
58.849560	28.139544	76.615758
58.447145	23.635562	76.620762
57.247007	31.664449	76.625767
56.537331	24.342630	76.630772
56.242133	19.670165	76.635777
55.570539	23.498988	76.640782
55.549774	17.302026	76.645786
54.061960	39.591164	76.650791
53.344704	30.258399	76.655796
53.118216	28.440240	76.660801
51.801934	28.125240	76.665806
51.350968	19.773433	76.670810
50.719995	28.473195	76.675815
50.262269	22.992461	76.680820
49.976491	27.426788	76.685825
49.008255	38.228768	76.690830
48.143651	32.158504	76.695834
47.600720	29.178164	76.700839
47.070336	21.942868	76.705844
45.979093	31.080312	76.710849
45.461649	33.750747	76.715854
45.049032	27.557935	76.720858
44.504984	22.603470	76.725863
44.166621	28.060145	76.730868
43.243128	27.677770	76.735873
42.658281	30.466187	76.740878
41.422001	29.554972	76.745882
40.458058	41.322924	76.750887
39.987352	27.294192	76.755892
39.799467	29.708640	76.760897
39.179878	32.305484	76.765902
38.456618	27.277104	76.770906
37.706677	29.494200	76.775911
37.415748	31.940854	76.780916
36.262582	23.169628	76.785921
35.516534	33.027862	76.790926
35.231657	28.768482	76.795930
34.543075	35.146750	76.800935
33.803080	34.618419	76.805940
33.143140	33.252590	76.810945
32.854706	34.391579	76.815950
31.839230	27.236812	76.820954
30.691283	36.444809	76.825959
30.320821	21.761442	76.830964
29.889429	23.194463	76.835969
29.339190	20.341449	76.840974
28.536043	23.363378	76.845978
27.707194	33.379898	76.850983
27.296207	24.804103	76.855988
25.914266	16.208147	76.860993
24.969233	27.764923	76.865998
25.082115	18.183074	76.871002
24.206604	25.190385	76.876007
24.012000	16.927004	76.881012
23.789962	19.504591	76.886017
22.807896	20.826757	76.891022
22.345164	15.707946	76.896026
20.962493	26.732145	76.901031
20.790633	15.968872	76.906036
20.063421	10.939558	76.911041
19.072171	13.928415	76.916046
18.218131	11.816132	76.921050
17.758455	15.609582	76.926055
16.991075	14.932664	76.931060
16.800707	15.015244	76.936065
16.415943	24.520965	76.941070
15.212587	15.882338	76.946074
14.394886	18.966515	76.951079
14.180240	18.970968	76.956084
13.443567	14.812047	76.961089
12.523302	17.240817	76.966094
12.103412	14.854284	76.971098
11.180176	15.652994	76.976103
10.087709	8.661913	76.981108
9.502667	16.884426	76.986113
9.081369	16.645882	76.991118
8.604284	12.456594	76.996122
8.072864	20.549133	77.001127
7.980941	14.040258	77.006132
7.111371	18.364285	77.011137
6.071515	17.729257	77.016142
4.987048	19.572377	77.021147
4.145787	16.668023	77.026151
3.472783	13.205409	77.031156
3.058629	14.460646	77.036161