Mon Mar 08 18:00:44 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.652832	101.582179	0.000000
-1.560576	79.500239	0.005005
-2.823180	53.047178	0.010010
-4.055216	14.708814	0.015014
-8.593783	8.171276	0.020019
-13.993140	10.945533	0.025024
-18.741757	0.026165	0.030029
-23.356209	-0.119047	0.035034
-27.553306	4.075070	0.040038
-30.896054	2.837640	0.045043
-34.920594	11.323410	0.050048
-38.197325	12.316253	0.055053
-42.167790	17.835123	0.060058
-45.718426	5.363829	0.065062
-49.431983	4.024732	0.070067
-53.778774	7.804392	0.075072
-57.217117	8.700042	0.080077
-60.926221	8.476706	0.085082
-64.565576	-6.370993	0.090086
-68.095156	-0.692194	0.095091
-72.267393	3.622609	0.100096
-75.861450	2.909445	0.105101
-79.727984	6.207267	0.110106
-83.319417	9.197863	0.115110
-86.914647	4.582046	0.120115
-91.332190	15.514896	0.125120
-94.886067	3.837387	0.130125
-98.689649	8.388302	0.135130
-101.955576	5.251151	0.140134
-105.656211	12.535787	0.145139
-109.718888	7.378010	0.150144
-113.286988	3.275132	0.155149
-117.358758	9.799004	0.160154
-121.273028	14.840689	0.165158
-124.675345	1.896441	0.170163
-128.955513	6.733171	0.175168
-131.891332	0.564608	0.180173
-136.051705	7.170453	0.185178
-139.562180	-0.901202	0.190182
-143.570019	-4.072873	0.195187
-147.739618	-1.338431	0.200192
-151.604693	-3.170419	0.205197
-155.796877	8.395187	0.210202
-159.053812	3.618271	0.215206
-162.614617	10.144259	0.220211
-166.331649	8.052133	0.225216
-170.124826	-1.240622	0.230221
-174.028509	2.427540	0.235226
-177.617358	0.518400	0.240230
-181.063725	7.459802	0.245235
-185.417099	2.067857	0.250240
-188.812225	1.630615	0.255245
-192.650087	9.495500	0.260250
-196.331659	1.602620	0.265254
-199.650174	4.543523	0.270259
-203.917993	7.889809	0.275264
-207.471156	9.600334	0.280269
-211.501685	7.160928	0.285274
-215.364448	8.372109	0.290278
-218.816521	3.385152	0.295283
-222.597445	15.877113	0.300288
-226.449760	7.890104	0.305293
-230.187041	17.156639	0.310298
-233.766576	12.067044	0.315302
-237.569444	9.395811	0.320307
-241.831496	10.793760	0.325312
-245.183596	8.727090	0.330317
-249.100478	19.854688	0.335322
-252.897597	9.152935	0.340326
-256.579839	4.861918	0.345331
-260.171383	-0.553711	0.350336
-263.930050	4.562703	0.355341
-268.346064	11.207995	0.360346
-271.734586	2.817465	0.365350
-274.966372	7.256882	0.370355
-278.954607	10.128177	0.375360
-283.028653	-2.724370	0.380365
-286.740515	7.277753	0.385370
-290.380311	-1.014293	0.390374
-294.092875	6.690399	0.395379
-298.086382	9.857448	0.400384
-301.717226	3.199244	0.405389
-305.764897	15.226139	0.410394
-309.577291	5.663875	0.415398
-313.018772	5.589013	0.420403
-316.874695	9.588814	0.425408
-320.224817	7.462013	0.430413
-324.743436	8.202493	0.435418
-327.935658	7.405060	0.440422
-331.621198	6.437233	0.445427
-334.983361	9.648631	0.450432
-338.744124	4.061446	0.455437
-343.210642	8.961410	0.460442
-346.833524	9.316090	0.465446
-350.690276	5.065697	0.470451
-354.903061	15.881156	0.475456
-358.415090	1.967643	0.480461
-361.950153	13.294639	0.485466
-365.732406	12.045845	0.490470
-369.354459	4.747696	0.495475
-373.011065	9.518409	0.500480
-376.521832	-3.110091	0.505485
-380.777123	9.664402	0.510490
-384.497611	7.563709	0.515494
-388.325973	3.660496	0.520499
-392.149119	9.178473	0.525504
-395.797633	5.115674	0.530509
-399.480333	7.673461	0.535514
-403.328784	3.027603	0.540518
-406.936100	4.403301	0.545523
-410.857427	-2.192577	0.550528
-414.554988	1.482477	0.555533
-418.352531	11.034863	0.560538
-422.309603	5.225277	0.565542
-425.974433	3.902640	0.570547
-429.461345	5.088839	0.575552
-433.240201	5.362903	0.580557
-437.325854	7.671287	0.585562
-440.596280	3.426763	0.590566
-444.528815	5.567210	0.595571
-448.472536	5.243170	0.600576
-452.198422	0.808050	0.605581
-455.961957	5.819880	0.610586
-459.880473	7.023009	0.615590
-463.397075	3.150556	0.620595
-467.490267	9.758839	0.625600
-470.553558	5.079167	0.630605
-474.652949	10.404851	0.635610
-478.805769	-3.521242	0.640614
-482.473254	-0.834877	0.645619
-486.265945	4.392960	0.650624
-489.763773	-3.569785	0.655629
-493.830341	4.369925	0.660634
-497.130314	5.445945	0.665638
-500.775186	1.594035	0.670643
-504.928939	7.500867	0.675648
-508.519371	-1.380588	0.680653
-512.622925	13.307904	0.685658
-516.175936	6.807914	0.690662
-519.863770	1.546836	0.695667
-523.733778	11.760637	0.700672
-527.316769	-0.253709	0.705677
-531.549156	2.478803	0.710682
-535.116854	0.669327	0.715686
-538.661594	3.386633	0.720691
-542.603348	6.902195	0.725696
-545.908646	-4.084177	0.730701
-550.102142	7.956923	0.735706
-553.583248	4.217705	0.740710
-557.477494	1.298245	0.745715
-561.589351	7.684166	0.750720
-565.013886	1.906455	0.755725
-568.774321	5.997050	0.760730
-572.567949	-0.628411	0.765734
-576.089914	2.183080	0.770739
-579.972787	7.537427	0.775744
-583.853199	-4.115508	0.780749
-587.914725	8.033879	0.785754
-591.453885	8.176865	0.790758
-595.236059	-1.328235	0.795763
-598.803891	-0.250284	0.800768
-602.487031	3.213023	0.805773
-606.544540	4.053831	0.810778
-610.104484	2.219576	0.815782
-614.035856	5.561713	0.820787
-617.870115	14.831690	0.825792
-621.448661	6.192934	0.830797
-625.148883	4.724877	0.835802
-628.740948	5.871397	0.840806
-632.634709	3.235827	0.845811
-636.788276	4.319107	0.850816
-640.473300	2.508036	0.855821
-644.469618	7.841187	0.860826
-647.920720	4.105203	0.865830
-651.314447	5.284721	0.870835
-655.075571	8.145576	0.875840
-658.726170	2.661160	0.880845
-662.713303	8.390253	0.885850
-666.834914	5.329113	0.890854
-670.360178	1.174518	0.895859
-674.403656	7.248512	0.900864
-677.890935	-4.019233	0.905869
-681.321655	3.074885	0.910874
-685.498370	-1.155361	0.915878
-689.530373	4.148873	0.920883
-693.162665	9.091211	0.925888
-696.901223	1.630862	0.930893
-700.259386	9.568096	0.935898
-703.918429	4.171830	0.940902
-707.809670	2.415894	0.945907
-711.848039	6.212089	0.950912
-715.512474	-0.288702	0.955917
-719.813366	-0.433793	0.960922
-723.428950	-1.167768	0.965926
-726.538195	5.846657	0.970931
-730.590301	13.025955	0.975936
-734.103359	4.048920	0.980941
-738.082167	12.952684	0.985946
-741.947816	2.106614	0.990950
-745.495339	4.282214	0.995955
-749.291039	2.645115	1.000960
-752.936372	1.826056	1.005965
-756.766837	9.217547	1.010970
-760.692560	1.069727	1.015974
-764.376924	2.464583	1.020979
-768.486227	1.620355	1.025984
-771.757023	-1.463038	1.030989
-775.949564	6.902528	1.035994
-779.559685	11.302151	1.040998
-783.094692	5.875150	1.046003
-787.133495	9.061281	1.051008
-790.753013	3.751875	1.056013
-794.557023	4.541449	1.061018
-798.487533	1.752764	1.066022
-802.182501	2.556460	1.071027
-805.881226	9.214211	1.076032
-809.135415	-4.137395	1.081037
-813.465388	9.162240	1.086042
-817.159307	13.920656	1.091046
-820.567046	5.308533	1.096051
-824.558961	6.418340	1.101056
-828.394639	-0.665154	1.106061
-832.186321	11.238068	1.111066
-835.692056	1.534653	1.116070
-839.442699	7.752914	1.121075
-843.623181	8.555439	1.126080
-847.197388	-1.919152	1.131085
-850.990155	10.037885	1.136090
-854.937409	13.296225	1.141094
-858.417337	0.849647	1.146099
-862.080920	14.120108	1.151104
-865.740968	1.443725	1.156109
-869.723569	16.231712	1.161114
-873.487165	-0.341966	1.166118
-877.262594	2.403255	1.171123
-881.322599	4.419721	1.176128
-884.532619	3.982267	1.181133
-888.905422	3.079454	1.186138
-892.242971	6.990983	1.191142
-896.222538	1.357700	1.196147
-899.727002	8.285722	1.201152
-903.098622	0.793860	1.206157
-907.517412	-1.456119	1.211162
-911.260774	4.273826	1.216166
-914.928040	8.354792	1.221171
-918.767784	9.147125	1.226176
-921.934507	-2.983582	1.231181
-926.007130	3.242136	1.236186
-929.922971	-2.166317	1.241190
-933.568628	-3.163231	1.246195
-937.611455	1.185967	1.251200
-941.288538	4.221482	1.256205
-945.260828	0.886238	1.261210
-948.741218	0.235069	1.266214
-952.188717	1.130312	1.271219
-956.487300	-2.551693	1.276224
-960.040856	-2.875766	1.281229
-963.898566	4.041023	1.286234
-967.372383	3.969129	1.291238
-971.003821	-3.514195	1.296243
-974.865071	6.834503	1.301248
-978.699373	-1.513624	1.306253
-982.540614	2.048081	1.311258
-986.345299	-0.820326	1.316262
-990.256665	-2.848526	1.321267
-993.825287	4.025235	1.326272
-997.488085	3.751802	1.331277
-1001.438662	5.566477	1.336282
-1005.505162	6.403099	1.341286
-1009.038394	5.424592	1.346291
-1012.712081	5.252270	1.351296
-1016.397728	0.198222	1.356301
-1020.414871	11.109645	1.361306
-1024.199117	7.050628	1.366310
-1027.500664	-1.592344	1.371315
-1031.397298	1.598267	1.376320
-1035.230263	1.151844	1.381325
-1038.965065	10.625742	1.386330
-1042.761714	4.264897	1.391334
-1046.492669	0.933806	1.396339
-1050.306392	1.285393	1.401344
-1053.900421	-3.179296	1.406349
-1058.165025	10.302682	1.411354
-1061.796528	2.018451	1.416358
-1065.241254	5.841709	1.421363
-1069.052627	12.025884	1.426368
-1073.057150	-3.386147	1.431373
-1076.705676	1.371707	1.436378
-1080.410475	5.030013	1.441382
-1084.127995	13.504620	1.446387
-1088.090075	7.627611	1.451392
-1091.378421	1.031007	1.456397
-1095.330673	11.074341	1.461402
-1099.232761	-3.526156	1.466406
-1103.199736	7.268566	1.471411
-1107.053934	5.765985	1.476416
-1110.032074	-1.025286	1.481421
-1113.746755	-0.396137	1.486426
-1117.869572	2.346691	1.491430
-1121.868876	9.415688	1.496435
-1125.901098	9.299322	1.501440
-1129.256657	7.376400	1.506445
-1133.306341	12.151211	1.511450
-1136.357892	10.345239	1.516454
-1140.271369	1.544874	1.521459
-1144.508994	5.387864	1.526464
-1148.256988	4.451812	1.531469
-1151.948585	4.708336	1.536474
-1155.769792	7.865008	1.541478
-1159.227455	7.191595	1.546483
-1163.121962	10.922957	1.551488
-1166.676690	5.403524	1.556493
-1170.485570	5.177390	1.561498
-1174.368257	-6.034174	1.566502
-1178.167281	-6.225604	1.571507
-1182.456866	0.363250	1.576512
-1185.664843	-0.047308	1.581517
-1189.471238	12.667747	1.586522
-1193.195234	5.418780	1.591526
-1196.713034	-2.402465	1.596531
-1200.676578	3.000470	1.601536
-1204.160954	-2.793498	1.606541
-1208.248820	1.423020	1.611546
-1212.461038	-2.955115	1.616550
-1215.865115	-3.315330	1.621555
-1219.455047	2.961372	1.626560
-1223.241108	5.901225	1.631565
-1227.094597	-0.803432	1.636570
-1230.957520	5.750352	1.641574
-1234.572307	6.527705	1.646579
-1238.483809	-0.593410	1.651584
-1241.841137	-11.072087	1.656589
-1245.706075	-0.772847	1.661594
-1249.803499	1.734346	1.666598
-1253.372174	5.271792	1.671603
-1257.149065	14.133038	1.676608
-1260.966724	3.407937	1.681613
-1264.834288	11.282378	1.686618
-1268.515502	7.118975	1.691622
-1272.146619	0.221120	1.696627
-1276.140554	12.718746	1.701632
-1279.533793	7.091650	1.706637
-1283.486061	11.565708	1.711642
-1287.259303	1.681914	1.716646
-1290.682340	3.950365	1.721651
-1295.228138	15.312679	1.726656
-1298.728858	4.234157	1.731661
-1302.250981	7.486695	1.736666
-1306.005332	5.121677	1.741670
-1309.140347	6.028931	1.746675
-1313.663038	11.378051	1.751680
-1316.883607	1.112550	1.756685
-1321.386495	6.075329	1.761690
-1325.480195	12.798663	1.766694
-1329.001286	8.340082	1.771699
-1332.610703	13.811131	1.776704
-1335.854365	5.228741	1.781709
-1339.615059	9.151853	1.786714
-1343.427833	10.680129	1.791718
-1346.999764	6.199754	1.796723
-1351.495692	9.567242	1.801728
-1355.053113	2.910027	1.806733
-1358.429584	6.762205	1.811738
-1362.315887	3.852300	1.816742
-1365.967028	-1.372269	1.821747
-1370.452389	4.049825	1.826752
-1373.700585	2.625719	1.831757
-1377.742037	3.312330	1.836762
-1381.368049	6.900147	1.841766
-1384.838215	6.706873	1.846771
-1388.743494	5.845275	1.851776
-1392.561797	3.454371	1.856781
-1396.677257	6.593886	1.861786
-1400.305066	10.098446	1.866790
-1403.527460	9.662114	1.871795
-1407.647796	6.157421	1.876800
-1411.508660	-3.786238	1.881805
-1414.966992	10.972269	1.886810
-1418.606938	4.511288	1.891814
-1422.469674	-6.936400	1.896819
-1426.555452	6.208495	1.901824
-1429.998044	-4.675692	1.906829
-1434.062115	-2.170364	1.911834
-1438.041035	-0.891289	1.916838
-1441.444082	-3.160946	1.921843
-1445.598839	7.308011	1.926848
-1448.934873	-2.623422	1.931853
-1452.935658	4.566199	1.936858
-1456.427589	3.947604	1.941862
-1460.119555	10.122738	1.946867
-1464.029386	17.334088	1.951872
-1467.920109	5.498308	1.956877
-1471.286977	5.542503	1.961882
-1475.125461	1.153900	1.966886
-1478.822737	1.645234	1.971891
-1483.120485	9.598365	1.976896
-1486.640065	-8.564925	1.981901
-1490.054305	2.085134	1.986906
-1494.336970	3.565903	1.991910
-1497.971835	1.459603	1.996915
-1501.658731	7.388586	2.006912
-1502.943919	7.238018	2.016909
-1500.536721	1.551037	2.026906
-1497.563203	3.732633	2.036902
-1495.214127	2.355904	2.046899
-1493.130375	9.021979	2.056896
-1491.583876	8.852163	2.066893
-1489.648008	3.739600	2.076890
-1487.676041	2.355371	2.086886
-1485.995520	3.548799	2.096883
-1484.195377	12.047619	2.106880
-1482.154314	9.485518	2.116877
-1479.857953	10.580339	2.126874
-1478.220224	7.444947	2.136870
-1476.349026	10.625693	2.146867
-1474.159014	6.383476	2.156864
-1472.461864	5.771140	2.166861
-1470.485666	3.255751	2.176858
-1468.899331	10.058339	2.186854
-1466.839396	7.261130	2.196851
-1464.714279	5.501881	2.206848
-1463.265972	12.323416	2.216845
-1461.356292	2.550978	2.226842
-1459.290152	3.922675	2.236838
-1457.209344	8.669306	2.246835
-1455.565293	7.356556	2.256832
-1453.885764	4.631320	2.266829
-1451.986164	4.267629	2.276826
-1449.677055	2.712612	2.286822
-1448.016005	-1.091211	2.296819
-1446.036743	6.941604	2.306816
-1444.068866	4.290205	2.316813
-1442.516041	6.415139	2.326810
-1440.691001	12.217976	2.336806
-1438.413791	3.346685	2.346803
-1436.836627	7.635566	2.356800
-1434.907747	3.455720	2.366797
-1432.929234	15.374362	2.376794
-1431.012402	12.506939	2.386790
-1429.194659	4.072367	2.396787
-1427.295541	6.228710	2.406784
-1425.344853	10.603057	2.416781
-1423.619902	9.035803	2.426778
-1421.754182	9.601223	2.436774
-1419.934603	11.973985	2.446771
-1417.857298	8.428793	2.456768
-1415.977180	7.997200	2.466765
-1414.207380	9.256913	2.476762
-1412.436842	8.219197	2.486758
-1410.319223	11.930534	2.496755
-1408.357784	13.806923	2.506752
-1406.685161	16.430587	2.516749
-1404.645635	7.177386	2.526746
-1402.954202	10.584336	2.536742
-1401.112123	15.795548	2.546739
-1399.193074	15.182477	2.556736
-1397.468410	20.685641	2.566733
-1395.516590	10.668084	2.576730
-1393.220266	10.604079	2.586726
-1391.581009	9.318981	2.596723
-1389.614386	9.876168	2.606720
-1387.843715	12.818878	2.616717
-1386.030837	15.145374	2.626714
-1383.927080	11.330720	2.636710
-1382.309220	6.134941	2.646707
-1380.313696	10.596885	2.656704
-1378.477175	10.132829	2.666701
-1376.251779	4.805063	2.676698
-1374.834285	7.539062	2.686694
-1372.974029	4.102864	2.696691
-1371.022057	6.609205	2.706688
-1369.204252	9.146499	2.716685
-1367.057273	10.884278	2.726682
-1365.221303	11.552398	2.736678
-1363.642300	9.596456	2.746675
-1361.509334	8.363398	2.756672
-1359.825212	9.128459	2.766669
-1357.778153	7.887051	2.776666
-1355.853225	13.988175	2.786662
-1353.929379	10.818120	2.796659
-1352.320818	6.907501	2.806656
-1350.397755	7.441694	2.816653
-1348.578418	11.767664	2.826650
-1346.395762	6.255718	2.836646
-1344.532615	0.302299	2.846643
-1342.897144	4.507706	2.856640
-1341.045322	12.139454	2.866637
-1339.009195	8.446187	2.876634
-1336.973251	14.821657	2.886630
-1335.346336	11.441782	2.896627
-1333.407035	6.035113	2.906624
-1331.455867	4.613293	2.916621
-1329.425992	5.758813	2.926618
-1327.734812	3.795992	2.936614
-1325.994290	6.263587	2.946611
-1324.049764	11.426887	2.956608
-1322.262872	8.259831	2.966605
-1320.055242	3.359686	2.976602
-1318.307907	2.974688	2.986598
-1316.500821	8.306830	2.996595
-1314.662222	4.902563	3.006592
-1312.557147	11.881185	3.016589
-1310.848870	11.153504	3.026586
-1309.132935	3.731602	3.036582
-1306.952654	6.520397	3.046579
-1305.188781	6.931689	3.056576
-1303.435289	10.931927	3.066573
-1301.619659	10.952843	3.076570
-1299.682717	7.479163	3.086566
-1297.869868	4.489546	3.096563
-1296.003967	7.639713	3.106560
-1293.914498	3.416909	3.116557
-1291.996335	4.214034	3.126554
-1290.150133	4.455849	3.136550
-1288.336096	7.184860	3.146547
-1286.433992	10.517132	3.156544
-1284.421601	16.121176	3.166541
-1282.558828	9.697344	3.176538
-1280.958143	5.715402	3.186534
-1279.021601	10.643184	3.196531
-1277.222948	7.687432	3.206528
-1275.334950	7.065222	3.216525
-1273.124566	11.434459	3.226522
-1271.394288	8.649124	3.236518
-1269.506317	6.983263	3.246515
-1267.712635	8.112955	3.256512
-1265.838600	5.716714	3.266509
-1263.973127	10.242207	3.276506
-1262.015265	8.852529	3.286502
-1260.143386	8.633955	3.296499
-1258.237038	15.934954	3.306496
-1256.345923	9.808177	3.316493
-1254.449367	12.538221	3.326490
-1252.829088	7.438451	3.336486
-1251.212276	12.497948	3.346483
-1248.948777	15.024017	3.356480
-1246.873241	12.387127	3.366477
-1245.039348	15.231416	3.376474
-1243.400737	8.129816	3.386470
-1241.210748	6.481962	3.396467
-1239.456421	14.235189	3.406464
-1237.761149	11.575476	3.416461
-1235.932797	8.393955	3.426458
-1233.764013	-1.145050	3.436454
-1231.978862	7.594803	3.446451
-1230.122892	9.005076	3.456448
-1228.378379	3.834918	3.466445
-1226.610694	14.778576	3.476442
-1224.299094	8.477173	3.486438
-1222.378210	11.648604	3.496435
-1220.871210	9.397968	3.506432
-1219.322364	19.337730	3.516429
-1217.062099	11.794048	3.526426
-1215.163792	17.651670	3.536422
-1213.386551	10.744217	3.546419
-1211.096472	11.822944	3.556416
-1209.449632	16.085056	3.566413
-1207.621742	19.105595	3.576410
-1205.738698	10.517044	3.586406
-1203.848619	2.284207	3.596403
-1202.169363	11.211554	3.606400
-1200.289722	10.342853	3.616397
-1198.336214	8.527618	3.626394
-1196.212285	8.202451	3.636390
-1194.554750	7.528762	3.646387
-1192.500106	8.656231	3.656384
-1190.663712	10.139141	3.666381
-1189.214664	10.932466	3.676378
-1186.886167	12.990312	3.686374
-1184.916865	8.287889	3.696371
-1183.134180	12.068821	3.706368
-1181.257400	13.527909	3.716365
-1179.432893	12.544890	3.726362
-1177.817365	14.893656	3.736358
-1175.808706	10.516515	3.746355
-1173.933504	9.656439	3.756352
-1172.023032	13.925345	3.766349
-1170.064262	15.778684	3.776346
-1168.077292	10.310832	3.786342
-1166.222239	10.890797	3.796339
-1164.586529	15.841549	3.806336
-1162.706718	15.568101	3.816333
-1160.691878	18.045622	3.826330
-1158.747403	19.875996	3.836326
-1157.035895	13.781184	3.846323
-1155.150980	12.043272	3.856320
-1153.246457	13.565838	3.866317
-1151.374787	21.006693	3.876314
-1149.294881	10.540937	3.886310
-1147.762027	14.349235	3.896307
-1145.857732	9.069887	3.906304
-1143.795885	12.689350	3.916301
-1141.772840	5.633679	3.926298
-1140.022132	7.572433	3.936294
-1138.061660	6.386120	3.946291
-1136.446087	18.011022	3.956288
-1134.126566	7.104324	3.966285
-1132.525720	8.189183	3.976282
-1130.661581	10.435054	3.986278
-1128.948014	5.457805	3.996275
-1127.135725	7.061461	4.006272
-1124.836520	8.899851	4.016269
-1123.348681	9.401228	4.026266
-1121.329997	7.011958	4.036262
-1119.140302	0.502793	4.046259
-1117.644747	1.613979	4.056256
-1115.788213	2.297954	4.066253
-1113.881534	6.336994	4.076250
-1111.910931	3.837005	4.086246
-1109.912591	11.813406	4.096243
-1108.359677	4.256663	4.106240
-1106.251636	4.693576	4.116237
-1104.377391	3.197407	4.126234
-1102.692738	8.413527	4.136230
-1100.660878	2.423825	4.146227
-1098.494424	10.932278	4.156224
-1097.170725	9.279450	4.166221
-1095.307667	2.977287	4.176218
-1093.083894	1.644685	4.186214
-1091.163046	7.918797	4.196211
-1089.626102	0.506724	4.206208
-1087.387719	0.371765	4.216205
-1085.566613	7.827074	4.226202
-1083.926040	2.122601	4.236198
-1081.933444	-0.044572	4.246195
-1079.809771	0.563545	4.256192
-1077.844163	-0.882481	4.266189
-1076.311053	3.862119	4.276186
-1074.709549	7.506331	4.286182
-1072.344950	-1.645449	4.296179
-1070.769030	-0.651296	4.306176
-1068.592783	2.345212	4.316173
-1066.786333	1.911472	4.326170
-1064.910880	-6.625230	4.336166
-1063.217726	-2.506208	4.346163
-1061.404801	-5.310927	4.356160
-1059.262733	0.900986	4.366157
-1057.493013	5.066188	4.376154
-1055.642573	0.463405	4.386150
-1053.766111	6.514128	4.396147
-1051.842397	4.474836	4.406144
-1050.211837	3.622409	4.416141
-1048.203709	9.241562	4.426138
-1046.244586	7.384502	4.436134
-1044.348223	3.022271	4.446131
-1042.507243	2.060408	4.456128
-1040.389844	0.976969	4.466125
-1038.626590	1.914341	4.476122
-1037.016965	-1.137313	4.486118
-1035.088177	-0.711139	4.496115
-1033.157287	3.898821	4.506112
-1031.361681	-8.630790	4.516109
-1029.505095	-2.433190	4.526106
-1027.314033	3.609870	4.536102
-1025.379706	1.971526	4.546099
-1023.855882	-0.218521	4.556096
-1021.989385	-1.546021	4.566093
-1020.044274	-4.750788	4.576090
-1018.022750	-4.050491	4.586086
-1016.225156	-4.616982	4.596083
-1014.145848	-5.918511	4.606080
-1012.516828	-0.036600	4.616077
-1010.732374	1.110557	4.626074
-1008.647578	0.177620	4.636070
-1006.927862	-6.720485	4.646067
-1004.864166	-7.332681	4.656064
-1003.099966	-4.633367	4.666061
-1001.373005	-5.302233	4.676058
-999.204143	-2.730785	4.686054
-997.507703	-1.029555	4.696051
-995.741006	0.483603	4.706048
-993.477818	-0.520479	4.716045
-991.714638	-2.140900	4.726042
-990.196142	1.914533	4.736038
-988.047265	0.867158	4.746035
-986.144125	-1.451416	4.756032
-984.296071	2.808683	4.766029
-982.568030	-2.769187	4.776026
-980.454010	5.231463	4.786022
-978.817998	-2.483749	4.796019
-976.980490	0.819641	4.806016
-974.704235	1.288194	4.816013
-973.115614	1.985126	4.826010
-971.430021	8.439066	4.836006
-969.500781	1.150643	4.846003
-967.492876	4.171010	4.856000
-965.577052	1.424116	4.865997
-963.785950	2.053940	4.875994
-961.496374	1.017249	4.885990
-959.727269	-0.354628	4.895987
-958.100858	1.995711	4.905984
-956.248596	6.608839	4.915981
-954.527798	-2.073581	4.925978
-952.345370	1.926240	4.935974
-950.463347	1.883129	4.945971
-948.545189	4.538924	4.955968
-947.033511	1.389308	4.965965
-944.972978	0.943455	4.975962
-943.372921	4.423785	4.985958
-941.027323	5.793897	4.995955
-939.002303	6.777910	5.005952
-937.474537	3.856248	5.015949
-935.874000	-1.799097	5.025946
-933.707534	-2.445032	5.035942
-931.447887	-2.509034	5.045939
-930.196681	3.267565	5.055936
-927.842402	-4.480356	5.065933
-926.228764	3.185098	5.075930
-924.089929	3.116736	5.085926
-922.113818	-0.795529	5.095923
-920.673539	-2.800051	5.105920
-918.917702	0.911174	5.115917
-917.143725	-2.054576	5.125914
-914.901054	6.943971	5.135910
-913.056512	4.664822	5.145907
-910.966398	-1.886662	5.155904
-909.113873	-5.179168	5.165901
-907.246128	5.164567	5.175898
-905.700891	0.787530	5.185894
-903.701229	5.613972	5.195891
-901.893089	4.971672	5.205888
-900.082740	3.463773	5.215885
-897.942769	7.232021	5.225882
-895.899172	-0.557779	5.235878
-894.251235	-0.252374	5.245875
-892.640436	0.142652	5.255872
-890.621135	3.631782	5.265869
-888.540813	7.587992	5.275866
-886.681212	1.403373	5.285862
-884.769469	4.244981	5.295859
-883.158668	3.597928	5.305856
-881.250500	5.825912	5.315853
-879.393114	8.046227	5.325850
-877.329272	1.810016	5.335846
-875.293770	5.564986	5.345843
-873.698596	0.666837	5.355840
-871.814174	6.089615	5.365837
-869.755771	4.613135	5.375834
-868.154375	3.838125	5.385830
-866.092608	3.466353	5.395827
-864.265001	5.918804	5.405824
-862.485557	14.159375	5.415821
-860.347346	13.000138	5.425818
-858.730889	7.918597	5.435814
-856.730433	12.666012	5.445811
-854.885124	6.835797	5.455808
-852.825738	9.175418	5.465805
-851.237060	10.879775	5.475802
-849.058746	14.032479	5.485798
-847.322096	12.867973	5.495795
-845.180168	12.574982	5.505792
-843.827311	12.322867	5.515789
-842.092176	11.117556	5.525786
-839.847439	16.556977	5.535782
-837.833978	11.830400	5.545779
-836.167860	8.957735	5.555776
-834.306983	11.779097	5.565773
-832.249022	13.114773	5.575770
-830.445642	5.331841	5.585766
-828.724853	10.245561	5.595763
-826.502289	9.290762	5.605760
-824.925839	9.236598	5.615757
-823.173165	9.967408	5.625754
-821.000978	10.905895	5.635750
-818.983571	6.764482	5.645747
-817.287766	6.972292	5.655744
-815.741947	14.373946	5.665741
-813.593685	5.288553	5.675738
-811.782297	12.673023	5.685734
-809.793819	11.010406	5.695731
-807.861402	9.961478	5.705728
-805.830175	10.875142	5.715725
-804.216646	16.169179	5.725722
-802.354967	22.153017	5.735718
-800.443045	14.419066	5.745715
-798.652703	16.064385	5.755712
-796.751440	19.671942	5.765709
-794.718632	20.905885	5.775706
-792.876509	20.041923	5.785702
-791.158991	13.559557	5.795699
-789.260759	14.592386	5.805696
-787.256248	17.297674	5.815693
-785.513094	12.448554	5.825690
-783.606161	8.986393	5.835686
-781.521318	16.087189	5.845683
-779.776976	18.117237	5.855680
-777.999286	14.912573	5.865677
-776.083747	16.926314	5.875674
-773.994105	18.166981	5.885670
-772.295134	12.039691	5.895667
-770.617183	13.330369	5.905664
-768.471377	11.563695	5.915661
-766.713470	16.552059	5.925658
-765.033097	10.615638	5.935654
-762.942029	14.862349	5.945651
-760.990904	11.009465	5.955648
-759.243079	9.412192	5.965645
-757.189325	11.620170	5.975642
-755.539917	16.090629	5.985638
-753.512750	13.409787	5.995635
-751.559655	17.800137	6.005632
-749.574020	23.091590	6.015629
-748.110835	13.806261	6.025626
-746.076208	14.683120	6.035622
-744.035647	11.510680	6.045619
-742.344115	17.256500	6.055616
-740.494357	12.087222	6.065613
-738.571211	15.664488	6.075610
-736.950516	13.841236	6.085606
-734.797881	11.148254	6.095603
-732.824494	14.592761	6.105600
-730.975336	16.658199	6.115597
-729.386066	14.874710	6.125594
-727.123945	15.342605	6.135590
-725.433531	15.780286	6.145587
-723.525790	18.570567	6.155584
-721.628136	14.661521	6.165581
-719.750925	9.955233	6.175578
-717.814155	14.166644	6.185574
-715.997928	11.390070	6.195571
-714.005752	11.280599	6.205568
-712.094232	8.604062	6.215565
-710.582495	8.392948	6.225562
-708.782986	10.298972	6.235558
-706.530897	9.386934	6.245555
-704.592403	11.289699	6.255552
-702.556770	10.469094	6.265549
-701.359645	14.713449	6.275546
-699.164087	10.311563	6.285542
-697.316743	6.072688	6.295539
-695.126073	12.851923	6.305536
-693.321771	11.496721	6.315533
-691.917542	14.179593	6.325530
-689.786934	12.963303	6.335526
-687.539508	11.055729	6.345523
-686.286455	12.780670	6.355520
-684.187970	10.194278	6.365517
-682.328255	10.794409	6.375514
-680.465967	13.658302	6.385510
-678.573658	7.797019	6.395507
-676.368513	7.822495	6.405504
-674.634465	4.369095	6.415501
-673.118670	10.921454	6.425498
-670.840615	10.790024	6.435494
-669.055306	11.799942	6.445491
-667.155269	9.174221	6.455488
-665.261795	7.967421	6.465485
-663.582984	6.412823	6.475482
-661.633605	11.173311	6.485478
-659.647341	11.508506	6.495475
-657.740312	10.744803	6.505472
-655.821313	7.801856	6.515469
-654.158329	9.601842	6.525466
-652.333335	14.499053	6.535462
-650.403504	5.060276	6.545459
-648.316712	13.735071	6.555456
-646.566889	6.543441	6.565453
-644.850604	13.472729	6.575450
-642.873992	17.808891	6.585446
-640.920706	12.228414	6.595443
-638.964920	10.253797	6.605440
-637.395658	12.351396	6.615437
-635.199031	14.111928	6.625434
-633.595004	15.033995	6.635430
-631.813107	8.530396	6.645427
-629.685030	10.213464	6.655424
-627.472169	10.842480	6.665421
-626.017906	12.284260	6.675418
-624.390504	6.129029	6.685414
-621.815940	11.152823	6.695411
-620.212116	8.962876	6.705408
-618.587507	5.926466	6.715405
-616.724832	14.506047	6.725402
-614.753142	13.485736	6.735398
-612.714444	6.508500	6.745395
-610.824575	8.307008	6.755392
-609.173513	8.234751	6.765389
-607.293783	7.102823	6.775386
-605.367823	11.901837	6.785382
-603.805696	10.735388	6.795379
-601.642098	7.071314	6.805376
-599.640428	5.068873	6.815373
-597.434160	4.224256	6.825370
-595.880214	10.701102	6.835366
-594.020291	6.802919	6.845363
-592.110850	16.109251	6.855360
-590.315903	15.200876	6.865357
-588.523868	16.291885	6.875354
-586.545348	12.927384	6.885350
-584.486087	8.545792	6.895347
-582.820776	8.220228	6.905344
-580.849567	11.166275	6.915341
-579.261272	12.454044	6.925338
-577.458473	4.819794	6.935334
-575.157654	16.872525	6.945331
-573.229906	6.218364	6.955328
-571.497596	6.281573	6.965325
-569.609039	12.212365	6.975322
-567.807217	22.189587	6.985318
-566.201514	13.271580	6.995315
-564.049484	15.839816	7.005312
-561.958787	15.828417	7.015309
-560.280446	12.131366	7.025306
-558.205192	9.881945	7.035302
-556.667214	15.543490	7.045299
-554.726973	18.233985	7.055296
-552.657227	9.762910	7.065293
-550.929847	7.914846	7.075290
-549.410793	12.973112	7.085286
-547.198617	9.383429	7.095283
-545.183149	6.139374	7.105280
-543.216261	12.829770	7.115277
-541.363854	9.218611	7.125274
-539.994416	19.347023	7.135270
-537.613934	17.100970	7.145267
-535.815343	14.273661	7.155264
-533.971502	11.546493	7.165261
-532.518486	14.029042	7.175258
-529.975066	12.661696	7.185254
-528.021344	13.919554	7.195251
-526.703797	14.650613	7.205248
-524.814608	18.168749	7.215245
-522.921881	11.467523	7.225242
-520.835768	15.735777	7.235238
-518.855880	15.551064	7.245235
-517.225281	10.278005	7.255232
-515.340479	13.301066	7.265229
-513.124593	9.878186	7.275226
-511.570366	12.571948	7.285222
-509.605450	19.354270	7.295219
-507.710444	3.408093	7.305216
-505.930923	9.267933	7.315213
-503.736357	4.073757	7.325210
-502.463185	2.547740	7.335206
-500.467062	5.156722	7.345203
-498.313810	7.538510	7.355200
-496.392827	2.741714	7.365197
-494.603751	11.522625	7.375194
-492.687215	7.418109	7.385190
-490.870466	4.995297	7.395187
-488.986888	10.456433	7.405184
-487.062045	12.277876	7.415181
-485.291037	8.177660	7.425178
-483.222998	10.107289	7.435174
-481.409200	14.809062	7.445171
-479.672414	6.283853	7.455168
-477.618482	6.429975	7.465165
-475.594601	9.249281	7.475162
-474.293932	9.390967	7.485158
-472.122881	14.891472	7.495155
-470.166094	11.606322	7.505152
-468.121408	8.826603	7.515149
-466.412463	8.424680	7.525146
-464.882467	8.225016	7.535142
-462.825086	9.632161	7.545139
-460.819446	9.787590	7.555136
-458.852951	9.218228	7.565133
-456.828921	12.256998	7.575130
-455.439107	7.592422	7.585126
-453.516936	5.637531	7.595123
-451.345231	6.998010	7.605120
-449.532623	3.145383	7.615117
-447.364621	2.861217	7.625114
-446.109098	8.070581	7.635110
-444.302298	13.128759	7.645107
-441.978587	10.053456	7.655104
-440.071899	4.881621	7.665101
-438.102454	7.678073	7.675098
-436.303683	11.581766	7.685094
-434.616514	9.246001	7.695091
-432.621128	4.749998	7.705088
-431.051121	5.854475	7.715085
-428.709864	5.987917	7.725082
-427.300974	3.537121	7.735078
-425.156768	9.210901	7.745075
-422.883201	6.587301	7.755072
-421.488252	6.958695	7.765069
-419.641509	2.306440	7.775066
-417.804304	3.560889	7.785062
-415.980595	8.130080	7.795059
-413.936043	0.717862	7.805056
-411.898860	3.291944	7.815053
-409.918084	7.970268	7.825050
-408.274356	8.188264	7.835046
-406.555870	10.473770	7.845043
-404.501696	7.106807	7.855040
-402.906412	4.776262	7.865037
-400.740685	5.441435	7.875034
-398.957184	6.281322	7.885030
-396.833935	8.843255	7.895027
-394.960012	7.704524	7.905024
-393.556406	5.229328	7.915021
-391.491561	6.861130	7.925018
-389.702786	3.582344	7.935014
-387.383277	5.902952	7.945011
-385.710405	4.109496	7.955008
-383.865096	7.309493	7.965005
-382.164927	-1.421380	7.975002
-380.162140	2.495570	7.984998
-378.396783	9.170921	7.994995
-376.332831	7.615028	8.004992
-374.532556	5.632293	8.014989
-372.561396	8.570631	8.024986
-370.811769	8.561748	8.034982
-368.707425	8.564128	8.044979
-367.043525	7.233163	8.054976
-365.439547	-0.211308	8.064973
-363.390559	-0.871129	8.074970
-361.236416	6.075317	8.084966
-359.619346	5.899713	8.094963
-357.708589	4.985653	8.104960
-355.663710	2.147577	8.114957
-353.780806	1.800064	8.124954
-351.976438	7.589746	8.134950
-350.442813	12.528982	8.144947
-348.337201	7.429665	8.154944
-345.949016	8.676734	8.164941
-344.568543	7.689449	8.174938
-342.655932	9.211389	8.184934
-340.581509	1.240255	8.194931
-339.170981	3.893916	8.204928
-336.936052	8.095948	8.214925
-335.087610	12.509680	8.224922
-333.352775	8.675866	8.234918
-331.405292	14.070094	8.244915
-329.122990	9.293107	8.254912
-327.529399	4.793435	8.264909
-325.777130	1.700519	8.274906
-323.813746	-2.097139	8.284902
-322.207194	7.003574	8.294899
-319.893995	8.439480	8.304896
-318.433433	9.270980	8.314893
-316.436167	11.998360	8.324890
-314.389237	8.263158	8.334886
-312.596553	5.580636	8.344883
-310.998188	10.110096	8.354880
-308.759727	4.785923	8.364877
-306.927863	3.008193	8.374874
-304.994417	3.263695	8.384870
-303.363711	0.673352	8.394867
-301.357241	4.536101	8.404864
-299.316136	-3.518100	8.414861
-297.505024	4.250522	8.424858
-295.637355	7.391758	8.434854
-293.995918	9.590173	8.444851
-291.973721	2.121618	8.454848
-290.053602	8.173923	8.464845
-288.066680	7.588808	8.474842
-286.379013	14.781894	8.484838
-284.563819	6.815863	8.494835
-282.773393	9.404184	8.504832
-280.631760	6.637565	8.514829
-278.686147	6.239050	8.524826
-277.090115	10.025231	8.534822
-275.260971	5.675884	8.544819
-272.901154	2.822342	8.554816
-271.335270	3.277065	8.564813
-269.144557	3.793108	8.574810
-267.630178	3.765007	8.584807
-265.814119	10.846036	8.594803
-263.785690	5.648583	8.604800
-261.878999	1.975282	8.614797
-260.142540	3.298038	8.624794
-258.425410	5.697552	8.634791
-256.454407	9.086008	8.644787
-254.499055	1.847621	8.654784
-252.450742	-3.738252	8.664781
-250.562618	-3.590734	8.674778
-248.892942	7.036257	8.684775
-247.090186	5.195322	8.694771
-244.853306	8.839771	8.704768
-243.253585	5.209160	8.714765
-241.181578	8.207303	8.724762
-239.500570	-0.610425	8.734759
-237.843361	0.871836	8.744755
-235.470413	3.714585	8.754752
-233.669241	-2.817081	8.764749
-231.740950	-6.615382	8.774746
-229.737712	0.134223	8.784743
-228.179378	0.530179	8.794739
-226.486683	1.282057	8.804736
-224.376453	-4.095784	8.814733
-222.287019	-1.251985	8.824730
-220.769165	-2.035338	8.834727
-218.936826	-1.432056	8.844723
-216.873550	-1.817721	8.854720
-215.031980	2.080893	8.864717
-213.043362	-4.256466	8.874714
-211.272708	1.522919	8.884711
-209.454686	-0.549369	8.894707
-207.438322	2.801889	8.904704
-205.827223	3.508383	8.914701
-203.646191	6.845998	8.924698
-202.491982	4.508602	8.934695
-200.067926	3.373804	8.944691
-198.000088	-1.015157	8.954688
-196.254455	4.896127	8.964685
-194.215652	2.817038	8.974682
-192.491450	-0.498671	8.984679
-190.648133	2.502852	8.994675
-188.788593	4.308119	9.004672
-186.966677	0.496825	9.014669
-185.158951	1.020378	9.024666
-183.223508	-1.473255	9.034663
-181.244066	1.910759	9.044659
-179.490342	-2.868583	9.054656
-177.416864	-6.710538	9.064653
-175.668299	-2.366005	9.074650
-174.010958	3.829383	9.084647
-171.859704	3.934974	9.094643
-169.910430	1.674404	9.104640
-168.054384	4.306024	9.114637
-166.134525	2.459093	9.124634
-164.242293	-4.184950	9.134631
-162.599189	2.909549	9.144627
-160.732252	-2.200473	9.154624
-158.763843	-3.706202	9.164621
-157.057909	-8.132115	9.174618
-155.042896	-1.509058	9.184615
-153.146760	2.150375	9.194611
-151.144767	-0.904899	9.204608
-149.173051	-1.058005	9.214605
-147.813728	3.656552	9.224602
-145.406954	5.660321	9.234599
-143.839076	1.722226	9.244595
-141.954000	5.178173	9.254592
-140.030354	-1.826126	9.264589
-138.026587	0.107745	9.274586
-136.374403	-1.137512	9.284583
-134.280679	3.483557	9.294579
-132.598875	-0.775863	9.304576
-130.705575	10.132911	9.314573
-128.539827	2.876833	9.324570
-126.769142	4.198963	9.334567
-125.036588	9.240823	9.344563
-122.828910	6.209593	9.354560
-121.373782	2.635287	9.364557
-119.492230	4.544463	9.374554
-117.536517	-0.143908	9.384551
-115.593751	-1.154464	9.394547
-113.762572	7.127421	9.404544
-111.782264	3.414066	9.414541
-110.013148	2.537008	9.424538
-107.969504	7.450300	9.434535
-106.379590	7.686562	9.444531
-104.310311	8.269497	9.454528
-102.497764	1.988731	9.464525
-100.742430	7.429602	9.474522
-98.637231	5.365260	9.484519
-96.683029	12.042289	9.494515
-95.216199	4.701958	9.504512
-93.013470	6.239391	9.514509
-91.300119	11.543286	9.524506
-89.251741	4.806486	9.534503
-87.459359	13.407216	9.544499
-85.717430	2.574615	9.554496
-83.886497	3.254013	9.564493
-81.677721	-0.393137	9.574490
-79.893273	11.775668	9.584487
-78.258559	9.824296	9.594483
-76.273295	5.560708	9.604480
-74.166402	1.524033	9.614477
-72.265075	4.011138	9.624474
-70.612555	-0.180413	9.634471
-68.782739	8.660670	9.644467
-66.942513	4.226020	9.654464
-64.919199	6.523147	9.664461
-62.776283	3.525986	9.674458
-61.483447	5.794386	9.684455
-59.507672	5.223867	9.694451
-57.115642	8.654274	9.704448
-55.405276	0.741436	9.714445
-53.619499	6.521694	9.724442
-51.863304	6.729886	9.734439
-50.069926	13.364718	9.744435
-48.072078	-1.940745	9.754432
-46.006451	6.798003	9.764429
-44.439023	9.027347	9.774426
-42.618035	3.504740	9.784423
-40.831686	14.831708	9.794419
-39.101886	8.546813	9.804416
-36.625022	9.476891	9.814413
-34.647803	10.972984	9.824410
-32.666201	10.794711	9.834407
-31.361427	2.806061	9.844403
-29.363751	14.023539	9.854400
-27.425300	7.992735	9.864397
-25.406107	8.844251	9.874394
-23.776422	8.155285	9.884391
-21.711506	9.938976	9.894387
-19.878755	7.984474	9.904384
-17.999924	7.607871	9.914381
-16.216847	10.865457	9.924378
-14.293040	10.091687	9.934375
-12.466333	7.607634	9.944371
-10.493223	7.266525	9.954368
-8.696183	9.209796	9.964365
-6.879773	0.297978	9.974362
-5.286012	12.550947	9.984359
-3.771732	35.750731	9.994355
-2.539323	78.776465	10.004352
-1.006711	128.390753	10.014349
0.000000	179.344145	10.019354
0.773421	221.374048	10.024359
1.461694	247.410132	10.029363
2.050322	264.670706	10.034368
2.096543	292.676379	10.039373
2.697897	299.260630	10.044378
2.714145	317.378958	10.049383
2.827303	326.302432	10.054387
3.668861	335.169656	10.059392
3.593824	347.813222	10.064397
3.514636	348.311783	10.069402
3.411294	354.683608	10.074407
3.452383	352.368628	10.079411
3.361739	351.790382	10.084416
3.600788	371.516423	10.089421
3.550356	367.771548	10.094426
3.613155	371.888647	10.099431
3.801957	376.805666	10.104435
3.672357	367.659738	10.109440
3.322825	372.222650	10.114445
3.950607	380.559449	10.119450
4.146273	397.196884	10.124455
4.082825	398.426221	10.129459
4.249350	394.083762	10.134464
4.286761	397.342323	10.139469
3.965317	386.381944	10.144474
4.427574	397.271436	10.149479
4.356536	391.564956	10.154483
4.322700	387.252879	10.159488
3.611324	395.642435	10.164493
4.467433	407.049435	10.169498
4.502516	404.003696	10.174503
4.341931	417.225519	10.179507
4.658582	414.003980	10.184512
4.531563	424.296776	10.189517
4.589389	432.262465	10.194522
4.440397	435.292145	10.199527
4.684011	432.127983	10.204531
4.759287	428.402466	10.209536
4.307623	435.317165	10.214541
4.801849	428.495485	10.219546
5.151765	430.176135	10.224551
4.726616	430.095942	10.229555
4.904422	428.326849	10.234560
4.589351	435.973547	10.239565
4.880526	443.086735	10.244570
4.925092	449.023423	10.249575
5.037315	461.824879	10.254579
5.742863	470.324371	10.259584
5.534139	464.310237	10.264589
5.258813	448.603681	10.269594
5.402671	446.655495	10.274599
5.629177	447.294536	10.279603
5.841610	440.990886	10.284608
5.384654	442.399686	10.289613
5.585764	439.732737	10.294618
5.401206	440.117220	10.299623
5.639416	443.914623	10.304627
5.438352	444.729095	10.309632
5.609583	436.946521	10.314637
5.987081	444.769766	10.319642
5.828035	443.368214	10.324647
5.936966	439.036504	10.329651
6.065615	440.470172	10.334656
5.778563	452.360743	10.339661
5.610541	449.811016	10.344666
5.758862	448.475557	10.349671
5.662934	449.755810	10.354675
6.221522	470.776169	10.359680
6.124458	483.609448	10.364685
6.208094	488.109613	10.369690
6.313655	483.970818	10.374695
6.344232	480.378575	10.379699
6.365167	466.816727	10.384704
6.041127	468.384103	10.389709
6.332365	477.864321	10.394714
6.453865	493.816678	10.399719
6.509394	490.516922	10.404723
6.900660	489.773496	10.409728
6.628878	480.981337	10.414733
6.951686	474.584372	10.419738
6.952433	471.946222	10.424743
6.441755	472.406376	10.429747
6.427229	464.643953	10.434752
6.317085	478.860735	10.439757
6.591830	489.982058	10.444762
6.343863	493.038575	10.449767
6.682289	499.844630	10.454771
6.745409	494.875232	10.459776
6.646744	502.760264	10.464781
7.049528	499.312078	10.469786
6.677352	508.675778	10.474791
6.557866	516.154126	10.479795
6.958041	525.262181	10.484800
6.934701	536.998794	10.489805
7.008196	540.888728	10.494810
7.347380	536.718963	10.499815
7.255763	537.610602	10.504819
7.522469	542.480558	10.509824
7.554314	550.486727	10.514829
7.737582	536.760148	10.519834
7.535610	536.486659	10.524839
7.436119	544.393923	10.529843
7.702540	546.009056	10.534848
7.870947	542.509933	10.539853
7.889148	535.548085	10.544858
7.530799	541.162718	10.549863
7.591691	543.256915	10.554867
7.805603	533.486805	10.559872
7.686875	544.732431	10.564877
7.695493	540.000371	10.569882
7.774885	546.016701	10.574887
7.160215	544.269913	10.579891
7.784045	557.391980	10.584896
7.997018	571.167803	10.589901
8.450414	564.781510	10.594906
7.942879	577.675612	10.599911
8.241242	570.222777	10.604915
8.678058	564.378455	10.609920
8.303187	581.504500	10.614925
8.245342	574.240945	10.619930
8.411430	571.798757	10.624935
8.399531	569.886437	10.629939
8.645874	565.056527	10.634944
8.636411	576.660070	10.639949
8.667873	571.727234	10.644954
8.682435	581.339960	10.649959
8.468431	578.403301	10.654963
8.917666	572.178520	10.659968
8.716070	582.393435	10.664973
8.814709	583.828750	10.669978
8.706029	590.908015	10.674983
8.390794	579.126471	10.679987
8.748447	577.702417	10.684992
8.506714	588.511950	10.689997
9.068759	582.191900	10.695002
8.568875	589.636341	10.700007
8.539645	583.259209	10.705011
9.189431	598.849873	10.710016
9.352147	608.891580	10.715021
9.490924	613.419260	10.720026
9.568836	599.558036	10.725031
9.159787	589.809978	10.730035
9.427580	590.581215	10.735040
9.283480	588.648977	10.740045
9.659514	593.790100	10.745050
9.355193	596.193295	10.750055
9.560903	608.686653	10.755059
9.699158	602.945129	10.760064
9.409690	609.881349	10.765069
9.754314	607.308176	10.770074
9.744070	618.866144	10.775079
9.676817	620.939791	10.780083
9.693057	620.636227	10.785088
9.535010	622.629736	10.790093
9.539847	621.168911	10.795098
9.972283	621.967506	10.800103
9.856390	621.539935	10.805107
10.245509	614.231878	10.810112
9.956062	618.676471	10.815117
9.820538	622.183442	10.820122
10.079303	623.116973	10.825127
10.390169	613.932175	10.830131
10.198662	618.690735	10.835136
9.727805	631.307793	10.840141
10.289061	613.900104	10.845146
10.122711	622.327438	10.850151
9.977269	631.030569	10.855155
10.617301	644.205326	10.860160
10.498927	658.597065	10.865165
10.589239	655.444691	10.870170
10.758022	651.380922	10.875175
10.789794	642.292661	10.880179
10.883543	625.330116	10.885184
10.746521	628.648090	10.890189
10.619916	623.555941	10.895194
10.378477	630.229039	10.900199
10.560184	645.910182	10.905203
10.891848	648.230872	10.910208
11.180300	655.805079	10.915213
11.143643	658.222364	10.920218
11.079558	659.180582	10.925223
10.969686	661.920212	10.930227
11.138933	655.924561	10.935232
10.988137	662.906498	10.940237
10.980650	653.080155	10.945242
11.249624	652.066062	10.950247
10.853112	655.270886	10.955251
11.511279	654.492767	10.960256
11.115049	657.267030	10.965261
11.460705	654.367249	10.970266
11.237858	657.448179	10.975271
11.350568	657.230154	10.980275
11.564692	658.210233	10.985280
11.267438	663.417767	10.990285
11.704939	652.862847	10.995290
11.659940	666.689369	11.000295
11.717252	686.500022	11.005299
12.015820	670.146590	11.010304
11.727653	667.729530	11.015309
11.760578	669.184797	11.020314
11.780812	680.036195	11.025319
12.080069	685.989129	11.030323
12.452159	679.912229	11.035328
11.769041	693.353266	11.040333
12.102979	672.569162	11.045338
12.536213	684.460157	11.050343
12.204390	671.988885	11.055347
12.371213	662.294010	11.060352
11.848151	663.051039	11.065357
12.180320	664.611544	11.070362
12.314458	677.401811	11.075367
12.270833	691.605037	11.080371
12.502847	685.145191	11.085376
12.534040	694.140314	11.090381
12.397146	683.743221	11.095386
12.397353	688.069093	11.100391
12.378551	690.470920	11.105395
12.719756	680.800260	11.110400
12.752643	685.999301	11.115405
12.706040	683.821260	11.120410
12.972758	685.002690	11.125415
12.910074	688.753532	11.130419
12.852113	686.578879	11.135424
12.522024	697.287465	11.140429
12.772986	689.157717	11.145434
13.001582	685.418720	11.150439
12.588003	696.038117	11.155443
12.752982	690.367992	11.160448
12.486502	699.333325	11.165453
13.016559	709.549906	11.170458
13.003099	713.690304	11.175463
13.237495	709.767445	11.180467
13.294614	720.040542	11.185472
13.045694	726.978234	11.190477
13.487781	713.170783	11.195482
13.648591	715.048791	11.200487
13.225482	717.981898	11.205491
13.428822	713.182453	11.210496
13.640045	716.104273	11.215501
13.565948	713.796568	11.220506
13.608936	718.440486	11.225511
13.140053	716.987397	11.230515
13.728454	713.779222	11.235520
13.413331	731.304354	11.240525
13.603479	730.517299	11.245530
14.123185	744.133975	11.250535
14.118349	754.871152	11.255539
14.034376	734.341278	11.260544
13.886798	738.900478	11.265549
13.982453	736.259757	11.270554
14.090668	749.000604	11.275559
13.947147	752.329105	11.280563
14.503045	743.065719	11.285568
14.158839	744.431330	11.290573
14.557745	749.352814	11.295578
14.271984	744.509940	11.300583
13.970661	749.729193	11.305587
14.380156	742.291663	11.310592
14.448154	749.601453	11.315597
14.707919	751.490492	11.320602
14.260013	752.659749	11.325607
14.330388	755.138829	11.330611
14.417926	753.734187	11.335616
14.736798	753.328734	11.340621
14.893087	754.683906	11.345626
14.635279	752.962175	11.350631
14.650501	756.661184	11.355635
14.613829	750.494905	11.360640
14.704119	749.838897	11.365645
15.053656	747.217607	11.370650
14.817436	753.344288	11.375655
14.804434	746.958188	11.380659
14.703797	750.447010	11.385664
14.546832	767.999001	11.390669
14.985650	773.899749	11.395674
15.165438	788.811779	11.400679
15.278330	779.719957	11.405683
15.498970	780.669041	11.410688
15.067872	789.553449	11.415693
15.443045	781.274525	11.420698
15.631215	782.258752	11.425703
15.692308	784.053323	11.430707
15.669572	785.041226	11.435712
15.580732	785.404142	11.440717
15.637561	788.743275	11.445722
16.010751	794.533071	11.450727
15.650441	782.192406	11.455731
15.608121	785.813865	11.460736
15.415753	794.324299	11.465741
15.828212	783.631349	11.470746
15.782526	783.749256	11.475751
15.577832	794.956745	11.480755
15.676153	785.818355	11.485760
15.443015	788.503550	11.490765
15.683518	791.311903	11.495770
15.620340	792.123324	11.500775
15.896443	811.048460	11.505779
15.996566	812.701187	11.510784
15.651269	824.317490	11.515789
16.278742	811.087525	11.520794
16.538788	821.159588	11.525799
16.311502	819.891889	11.530803
16.464839	809.744890	11.535808
16.469422	816.042931	11.540813
16.552343	816.720662	11.545818
16.565425	823.662345	11.550823
16.660956	821.210869	11.555827
16.767782	816.395244	11.560832
16.540188	829.114026	11.565837
16.712149	811.642032	11.570842
16.666976	820.815000	11.575847
16.325200	823.407138	11.580851
16.661013	818.233281	11.585856
16.735609	831.525205	11.590861
16.899952	821.909470	11.595866
16.637556	823.446549	11.600871
16.676719	824.055563	11.605875
16.831321	839.031588	11.610880
16.803019	858.283678	11.615885
17.043546	847.540831	11.620890
17.101771	842.619405	11.625895
17.244741	854.326595	11.630899
17.300992	846.251471	11.635904
17.027221	861.333691	11.640909
17.243507	855.365150	11.645914
17.072948	850.491250	11.650919
16.950198	853.070537	11.655923
17.536055	841.450997	11.660928
17.175677	847.643253	11.665933
17.515448	852.454351	11.670938
17.840117	844.505156	11.675943
17.337298	845.285774	11.680947
17.784749	855.327971	11.685952
17.789582	868.621595	11.690957
18.195362	855.769158	11.695962
17.893688	849.216159	11.700967
17.753791	851.962189	11.705971
18.084007	840.526930	11.710976
17.366315	862.063669	11.715981
18.241732	861.558408	11.720986
18.340276	868.063843	11.725991
17.818686	856.721852	11.730995
18.344278	861.446544	11.736000
18.166412	871.329859	11.741005
18.279250	858.636111	11.746010
18.433610	867.835632	11.751015
18.112918	858.141110	11.756019
18.398646	846.512662	11.761024
17.943799	859.409646	11.766029
18.418140	865.585475	11.771034
18.734398	871.613049	11.776039
18.713541	884.500762	11.781043
18.516194	877.196224	11.786048
18.540309	882.169646	11.791053
18.850830	869.849649	11.796058
18.890888	881.395073	11.801063
18.745086	885.712753	11.806067
19.026727	865.531247	11.811072
18.555640	869.845608	11.816077
18.930372	874.540747	11.821082
19.139114	873.861111	11.826087
18.987355	872.455199	11.831091
18.989404	862.928402	11.836096
18.759623	875.267514	11.841101
19.116587	872.469970	11.846106
18.797758	877.157455	11.851111
18.901102	884.994704	11.856115
19.458931	871.607052	11.861120
19.290208	884.843213	11.866125
19.074495	882.010846	11.871130
18.900992	879.137053	11.876135
18.540877	882.467012	11.881139
19.239183	882.384251	11.886144
19.481203	907.486574	11.891149
19.502840	905.152530	11.896154
19.588080	906.006520	11.901159
19.471303	911.822470	11.906163
19.556009	907.339938	11.911168
19.507389	914.359317	11.916173
19.702971	912.726108	11.921178
19.318434	914.954484	11.926183
19.912403	913.182038	11.931187
19.909202	909.151936	11.936192
19.597393	922.865132	11.941197
19.981167	912.635575	11.946202
20.027542	915.839205	11.951207
19.751753	916.763394	11.956211
20.010581	913.943646	11.961216
19.917506	909.656632	11.966221
20.065420	920.022627	11.971226
20.110983	935.517634	11.976231
20.315567	934.994782	11.981235
20.514438	930.837823	11.986240
20.368361	939.257376	11.991245
20.538426	933.269366	11.996250
20.371118	941.900473	12.001255
20.321757	936.521493	12.006259
20.600486	933.047260	12.011264
20.455822	940.555074	12.016269
20.623494	928.360318	12.021274
20.795284	930.820099	12.026279
20.471232	933.582900	12.031283
20.431152	930.120092	12.036288
20.477850	938.978848	12.041293
20.630121	934.140166	12.046298
20.894887	929.699874	12.051303
20.344712	939.530649	12.056307
20.757446	929.673367	12.061312
20.943160	939.306343	12.066317
20.679450	937.905665	12.071322
20.826138	931.694294	12.076327
20.795966	926.739627	12.081331
20.814253	912.274156	12.086336
20.406100	914.637191	12.091341
20.495035	909.892199	12.096346
20.462072	906.708969	12.101351
20.851013	909.548866	12.106355
20.971946	907.946488	12.111360
20.721341	912.500095	12.116365
20.882554	915.008871	12.121370
21.067362	905.120147	12.126375
20.478961	918.787565	12.131379
20.602711	905.541658	12.136384
20.460257	910.929602	12.141389
20.458323	912.354181	12.146394
20.254923	905.612010	12.151399
20.164717	916.643632	12.156403
20.572651	914.057155	12.161408
20.526193	916.572245	12.166413
20.763398	912.100083	12.171418
20.602712	916.842785	12.176423
20.600831	914.499874	12.181427
20.697621	905.229184	12.186432
20.399131	920.883133	12.191437
20.552192	920.992996	12.196442
20.624297	908.564331	12.201447
20.405161	915.831688	12.206451
20.866557	923.197097	12.211456
20.458008	921.242334	12.216461
20.540859	917.113346	12.221466
20.732599	926.218630	12.226471
20.709856	924.757442	12.231475
20.971888	924.458826	12.236480
20.669665	928.560183	12.241485
20.826360	919.478634	12.246490
21.005712	920.314461	12.251495
20.754931	925.134615	12.256499
20.762887	920.177023	12.261504
21.056014	924.388436	12.266509
20.894311	917.150735	12.271514
20.594301	924.044628	12.276519
20.517252	932.349084	12.281523
20.693698	916.692970	12.286528
20.696539	924.402762	12.291533
20.819297	929.866689	12.296538
20.514983	921.158299	12.301543
20.458693	918.904494	12.306547
20.738832	918.210313	12.311552
20.737280	923.971619	12.316557
20.783352	919.030026	12.321562
20.315585	903.557102	12.326567
20.474056	911.448654	12.331571
20.819778	917.088334	12.336576
20.687741	922.670170	12.341581
20.973601	905.935286	12.346586
20.889377	898.070203	12.351591
20.615492	896.108159	12.356595
20.616704	895.223492	12.361600
20.684515	897.904863	12.366605
20.582002	891.938266	12.371610
20.432293	893.570924	12.376615
20.522862	898.642566	12.381619
20.679358	893.547747	12.386624
20.354792	903.233700	12.391629
20.288410	901.522422	12.396634
20.403182	908.023710	12.401639
20.758984	922.972463	12.406643
20.852798	907.148182	12.411648
20.382370	912.914878	12.416653
20.539854	906.323313	12.421658
20.852167	912.190678	12.426663
20.760463	905.824945	12.431667
20.599958	901.690619	12.436672
20.449959	898.844613	12.441677
20.717125	899.369955	12.446682
20.952510	906.260451	12.451687
20.872510	904.286406	12.456691
20.672877	907.814710	12.461696
20.558621	904.892037	12.466701
21.227160	901.991175	12.471706
20.886942	913.267681	12.476711
20.614716	916.167298	12.481715
20.754707	907.810692	12.486720
20.587234	906.859885	12.491725
20.533879	911.219600	12.496730
20.593280	905.749164	12.501735
20.493075	913.494310	12.506739
21.091960	906.739300	12.511744
20.394193	912.811924	12.516749
20.702601	908.617000	12.521754
20.690846	906.485408	12.526759
20.473339	911.284481	12.531763
20.505368	905.496701	12.536768
20.304518	910.868726	12.541773
20.611634	917.235258	12.546778
20.755113	909.739143	12.551783
20.384616	910.356727	12.556787
20.444068	907.265993	12.561792
20.335204	913.381891	12.566797
20.502044	899.988762	12.571802
20.745494	908.179006	12.576807
20.605722	908.274071	12.581811
20.738828	909.122005	12.586816
20.764281	913.297256	12.591821
20.763375	908.248038	12.596826
20.746190	905.738830	12.601831
20.476973	915.141563	12.606835
21.268834	910.981498	12.611840
20.885960	916.830429	12.616845
20.617513	896.796542	12.621850
20.509986	897.198712	12.626855
20.054439	892.710886	12.631859
20.664727	899.402807	12.636864
20.469308	912.524975	12.641869
20.891235	909.633482	12.646874
21.173457	915.616038	12.651879
20.740427	901.590004	12.656883
20.792009	891.987476	12.661888
20.574235	894.733320	12.666893
20.390478	885.269260	12.671898
20.676801	878.892133	12.676903
19.834956	889.408082	12.681907
20.509734	895.484143	12.686912
20.817517	908.215379	12.691917
20.442795	915.233151	12.696922
20.845139	916.202152	12.701927
20.485776	911.011402	12.706931
20.779617	915.366206	12.711936
20.337836	921.976769	12.716941
20.289525	917.464985	12.721946
20.614065	919.553459	12.726951
20.272803	925.040928	12.731955
20.487917	920.852995	12.736960
20.489316	918.457519	12.741965
20.981393	922.353338	12.746970
20.789968	920.819702	12.751975
20.887596	921.340544	12.756979
20.772646	920.699917	12.761984
20.582963	926.360337	12.766989
20.397053	929.990540	12.771994
21.141451	921.539103	12.776999
20.706836	918.517707	12.782003
20.333270	899.203930	12.787008
20.336722	905.987910	12.792013
20.672077	913.813403	12.797018
20.830668	920.295092	12.802023
20.416356	927.073170	12.807027
20.673319	917.247050	12.812032
20.622899	930.680435	12.817037
20.700172	927.627857	12.822042
20.750288	917.787417	12.827047
20.360829	911.492827	12.832051
20.570047	905.176873	12.837056
20.615483	923.322843	12.842061
20.818071	922.137965	12.847066
20.817131	909.765105	12.852071
20.532851	908.804542	12.857075
20.708534	897.991573	12.862080
20.419387	910.551503	12.867085
20.724019	907.161458	12.872090
20.601744	911.473816	12.877095
20.306223	912.796982	12.882099
20.616103	900.224740	12.887104
20.687491	914.692126	12.892109
20.611339	915.493007	12.897114
20.765295	903.185338	12.902119
20.644128	903.359440	12.907123
20.897075	894.702541	12.912128
21.026213	905.248145	12.917133
20.755596	908.168005	12.922138
20.928261	901.928849	12.927143
20.688812	896.953952	12.932147
21.129653	892.446164	12.937152
20.856313	901.948898	12.942157
20.849136	899.026494	12.947162
20.551166	894.226519	12.952167
20.380689	910.118668	12.957171
20.827658	896.322882	12.962176
20.491651	903.678262	12.967181
20.521451	908.642901	12.972186
20.874010	905.152169	12.977191
20.604923	889.775309	12.982195
20.727525	874.582006	12.987200
20.613770	878.274808	12.992205
20.504722	877.295761	12.997210
21.120776	875.253282	13.002215
20.345218	873.825433	13.007219
20.632402	872.289586	13.012224
20.458204	868.007638	13.017229
20.540937	871.430971	13.022234
20.659841	864.298357	13.027239
20.370217	866.519473	13.032243
20.555378	890.509584	13.037248
20.622461	901.667500	13.042253
20.804461	891.115313	13.047258
20.532620	888.515831	13.052263
20.307699	877.509719	13.057267
20.867594	892.955765	13.062272
20.751570	902.545375	13.067277
20.539389	890.671442	13.072282
20.539492	877.946770	13.077287
20.789351	881.341873	13.082291
20.769819	878.703729	13.087296
20.655772	880.381161	13.092301
20.826211	866.451306	13.097306
21.021498	867.724573	13.102311
20.963912	876.038510	13.107315
20.803010	873.733584	13.112320
20.702553	874.486299	13.117325
20.752089	872.900043	13.122330
20.780792	878.296947	13.127335
20.467174	877.541346	13.132339
20.821767	880.801468	13.137344
20.721436	882.591835	13.142349
20.690728	877.220941	13.147354
20.801245	872.961392	13.152359
20.738651	871.654803	13.157363
20.692087	869.413647	13.162368
20.467265	857.027653	13.167373
20.415461	863.954472	13.172378
20.851493	867.960143	13.177383
20.622713	866.486089	13.182387
20.898320	849.306613	13.187392
20.471714	850.130269	13.192397
20.346448	851.599746	13.197402
20.626595	853.351503	13.202407
20.452216	862.863659	13.207411
20.448348	867.218622	13.212416
20.779323	870.618132	13.217421
20.662617	875.096753	13.222426
20.923572	876.428936	13.227431
20.504433	867.168016	13.232435
20.535565	847.990040	13.237440
20.404056	862.606434	13.242445
20.670127	862.332407	13.247450
20.956392	865.876246	13.252455
20.653624	857.284347	13.257459
20.493985	845.692239	13.262464
20.516330	845.974343	13.267469
20.422126	850.772654	13.272474
20.561317	859.607148	13.277479
20.715900	880.763509	13.282483
20.772433	868.575489	13.287488
20.454345	863.531143	13.292493
20.386380	856.843090	13.297498
20.791231	860.156695	13.302503
20.661626	874.345427	13.307507
20.704195	859.962871	13.312512
20.358957	862.869392	13.317517
20.647340	870.577769	13.322522
20.795181	878.597159	13.327527
20.343715	872.842351	13.332531
20.692530	868.877545	13.337536
20.857469	873.114119	13.342541
20.553757	863.494158	13.347546
20.793650	856.178241	13.352551
20.191096	859.338698	13.357555
20.550449	862.758912	13.362560
20.397105	867.440500	13.367565
20.507957	874.965877	13.372570
20.819303	881.066780	13.377575
20.592597	889.972267	13.382579
20.857363	881.841788	13.387584
20.159263	879.819669	13.392589
20.340226	886.816610	13.397594
20.578183	876.288625	13.402599
20.554103	886.685182	13.407603
20.490911	888.742449	13.412608
20.734740	891.441478	13.417613
20.693897	885.447701	13.422618
20.791746	883.175624	13.427623
20.570181	890.437048	13.432627
20.686760	881.910720	13.437632
20.458466	893.221400	13.442637
20.562561	891.318924	13.447642
20.785620	882.469672	13.452647
20.262540	889.351817	13.457651
20.539508	895.918696	13.462656
20.517448	893.421306	13.467661
20.465503	888.271422	13.472666
20.636641	895.405558	13.477671
20.499938	899.455275	13.482675
20.499598	886.173982	13.487680
20.340303	898.642226	13.492685
20.392756	893.865210	13.497690
20.714813	891.112656	13.502695
20.425947	900.789759	13.507699
20.646992	885.158106	13.512704
20.532781	892.000271	13.517709
20.578103	886.967343	13.522714
20.546317	895.520035	13.527719
20.339911	901.936923	13.532723
20.698665	903.807041	13.537728
20.615237	897.193978	13.542733
20.628927	903.214628	13.547738
20.575772	906.043031	13.552743
20.499271	903.683637	13.557747
20.391848	891.640025	13.562752
20.558124	897.536984	13.567757
20.493702	903.917035	13.572762
20.657755	892.287456	13.577767
20.650842	898.797109	13.582771
20.698715	889.898521	13.587776
20.776710	895.585625	13.592781
20.506567	903.933478	13.597786
20.599526	901.695296	13.602791
20.418508	899.144408	13.607795
20.897335	892.388052	13.612800
20.476262	900.807287	13.617805
20.616192	897.459283	13.622810
20.770180	899.852509	13.627815
20.619456	901.792847	13.632819
20.956758	904.210454	13.637824
20.456747	901.950149	13.642829
20.420504	896.360926	13.647834
20.888933	893.067766	13.652839
20.160026	902.080168	13.657843
20.601531	901.478527	13.662848
20.552569	899.182553	13.667853
20.530958	900.922518	13.672858
20.838074	891.309197	13.677863
20.936551	908.981472	13.682867
20.876112	905.638615	13.687872
20.656762	898.481083	13.692877
20.736133	903.311653	13.697882
20.946991	905.574381	13.702887
21.048946	911.830124	13.707891
21.138592	903.550938	13.712896
20.872949	894.019506	13.717901
20.804445	880.772745	13.722906
20.703773	873.247778	13.727911
20.109197	882.757578	13.732915
20.305065	883.147629	13.737920
20.592029	873.340408	13.742925
20.763397	888.730142	13.747930
20.743026	877.528973	13.752935
20.777280	884.347455	13.757939
20.845012	873.628995	13.762944
20.589334	876.038670	13.767949
20.655402	876.443115	13.772954
20.722860	859.992285	13.777959
20.560619	874.466930	13.782963
20.784921	877.254230	13.787968
20.657747	873.010513	13.792973
20.258512	881.528759	13.797978
20.407896	876.148066	13.802983
20.311990	877.379465	13.807987
20.558057	868.083413	13.812992
20.458411	884.814244	13.817997
20.523713	901.129265	13.823002
20.962825	888.175286	13.828007
20.518228	899.052099	13.833011
20.549998	886.282944	13.838016
20.640848	882.324584	13.843021
20.443928	880.514275	13.848026
20.668728	892.378761	13.853031
20.523277	894.933291	13.858035
20.822262	900.097853	13.863040
20.583100	898.377861	13.868045
20.665877	894.360859	13.873050
20.694521	877.723805	13.878055
20.497803	897.731387	13.883059
20.723661	888.326577	13.888064
20.623010	879.541574	13.893069
20.617177	878.268511	13.898074
20.577413	884.160479	13.903079
20.313430	895.467391	13.908083
20.544373	890.649293	13.913088
20.670107	898.978160	13.918093
20.835463	889.062586	13.923098
20.878768	880.939044	13.928103
20.697505	894.735475	13.933107
20.872639	893.357851	13.938112
20.564746	888.844899	13.943117
20.652292	883.748465	13.948122
20.660544	878.342970	13.953127
20.609823	888.545075	13.958131
20.773376	889.963759	13.963136
20.924893	882.581498	13.968141
20.801702	885.823205	13.973146
20.841807	881.319409	13.978151
20.750252	888.249425	13.983155
20.785664	873.648793	13.988160
20.754544	883.650641	13.993165
20.580100	877.282347	13.998170
20.514879	889.789197	14.003175
20.452095	894.916837	14.008179
20.826204	875.980600	14.013184
20.540135	887.563852	14.018189
20.523476	886.691219	14.023207
21.019726	881.136736	14.028224
20.852559	888.964066	14.033242
20.581807	872.299228	14.038259
20.304087	877.224725	14.043277
20.639262	880.339489	14.048295
20.918341	883.858020	14.053312
20.702641	895.340849	14.058330
20.881477	886.466079	14.063347
20.625167	892.051966	14.068365
20.571025	892.908672	14.073383
20.786056	884.360030	14.078400
20.549980	888.711041	14.083418
20.596868	886.056457	14.088435
20.454550	894.240041	14.093453
20.595206	890.496150	14.098471
20.459101	888.039062	14.103488
20.396787	895.146547	14.108506
21.040703	895.108569	14.113523
20.839953	909.684663	14.118541
20.621437	921.757833	14.123559
21.041422	922.645883	14.128576
20.869094	922.355855	14.133594
20.909162	931.260686	14.138611
21.097269	920.599071	14.143629
21.041988	918.275375	14.148647
21.398593	928.153734	14.153664
21.030377	937.789063	14.158682
21.059282	921.925789	14.163699
21.164572	926.407978	14.168717
21.144764	932.862203	14.173735
21.117004	925.618519	14.178752
20.919613	932.654760	14.183770
20.929491	930.907395	14.188787
21.106800	928.024367	14.193805
20.841390	924.104566	14.198823
20.917113	930.477487	14.203840
20.971231	932.806551	14.208858
21.307528	923.189360	14.213875
21.177177	937.757401	14.218893
20.853243	939.146340	14.223911
21.137981	956.158689	14.228928
21.106533	964.312045	14.233946
21.383120	955.670175	14.238963
21.433702	965.808151	14.243981
21.314057	958.026985	14.248999
21.496700	961.773270	14.254016
21.142009	965.627280	14.259034
21.442717	960.896745	14.264051
21.661099	954.628369	14.269069
21.381676	962.130730	14.274087
21.227147	960.617219	14.279104
21.048087	965.622962	14.284122
21.306368	962.649936	14.289139
21.713983	961.443160	14.294157
21.740097	963.293786	14.299175
22.024826	958.255920	14.304192
21.743785	962.079306	14.309210
21.657149	961.903022	14.314227
22.002201	967.221568	14.319245
21.490327	967.715564	14.324263
21.642614	958.610608	14.329280
21.816228	966.231047	14.334298
21.789298	972.442611	14.339315
21.694929	965.593342	14.344333
21.504148	966.289377	14.349351
21.726907	960.745452	14.354368
21.854026	972.610956	14.359386
21.662381	969.712835	14.364403
21.832778	967.496279	14.369421
21.635617	960.696440	14.374439
21.719182	971.124881	14.379456
21.800488	986.201896	14.384474
21.967577	988.997433	14.389491
22.084890	996.104632	14.394509
22.314836	987.029743	14.399527
22.146579	967.082906	14.404544
22.119937	974.082496	14.409562
21.997905	967.464149	14.414579
22.249184	957.940718	14.419597
21.866428	963.858253	14.424615
22.011495	968.145352	14.429632
21.980293	968.568975	14.434650
22.091981	964.584299	14.439667
22.264346	977.776491	14.444685
22.121321	982.123699	14.449703
22.333375	974.410741	14.454720
22.173731	970.837420	14.459738
22.055025	972.665528	14.464755
22.199501	975.397030	14.469773
22.288694	992.009610	14.474791
22.338719	990.732452	14.479808
22.118240	995.968178	14.484826
22.379991	996.323056	14.489843
22.475697	995.713429	14.494861
22.126632	1000.846971	14.499879
22.717463	984.401656	14.504896
22.583085	994.035906	14.509914
22.322809	987.236682	14.514931
22.464975	979.983172	14.519949
22.480259	992.113490	14.524967
22.579302	990.125385	14.529984
22.249562	981.915253	14.535002
22.633571	985.830772	14.540019
22.919908	995.522188	14.545037
22.483223	987.522589	14.550055
22.502189	967.102306	14.555072
22.840416	975.407488	14.560090
22.530524	982.485291	14.565107
22.565098	965.389409	14.570125
22.391795	971.476457	14.575143
22.552841	982.204002	14.580160
22.932006	992.232961	14.585178
22.607170	998.660361	14.590195
22.816855	994.537353	14.595213
22.894928	1003.481784	14.600231
22.963133	989.370781	14.605248
22.694046	979.983813	14.610266
22.541277	981.930610	14.615283
22.762968	986.589305	14.620301
22.568706	992.557010	14.625319
22.683736	995.769831	14.630336
22.527280	1003.302937	14.635354
22.794702	993.839828	14.640371
22.851081	997.648732	14.645389
22.750877	993.509084	14.650407
22.932627	985.126137	14.655424
23.048047	998.782027	14.660442
23.147788	995.736754	14.665459
23.121060	993.059286	14.670477
23.028654	1001.623499	14.675495
23.222936	986.513986	14.680512
22.970130	999.044138	14.685530
22.937198	984.925676	14.690547
22.915372	999.339618	14.695565
22.739232	1001.143857	14.700583
23.321570	993.892493	14.705600
23.344154	992.509602	14.710618
23.069235	996.862121	14.715635
23.088504	991.920065	14.720653
23.003669	989.014342	14.725671
23.053341	991.951302	14.730688
23.432221	1020.802827	14.735706
23.537168	1023.356603	14.740723
23.625637	1000.611303	14.745741
23.299976	992.347033	14.750759
23.332408	990.756509	14.755776
23.311497	991.524551	14.760794
23.062049	997.741729	14.765811
23.433783	1015.353743	14.770829
23.410141	1022.713095	14.775847
23.957449	1019.500480	14.780864
23.641024	994.790597	14.785882
23.281639	989.811408	14.790899
23.836604	990.935906	14.795917
23.536484	997.916205	14.800935
23.519851	988.525145	14.805952
23.467400	992.945999	14.810970
23.730988	1001.555679	14.815987
23.567127	993.334814	14.821005
23.726006	998.764861	14.826023
23.776623	1007.625586	14.831040
23.468265	996.439067	14.836058
23.652204	1011.712094	14.841075
23.965212	1006.742059	14.846093
23.809963	1023.478604	14.851111
23.808295	1002.446518	14.856128
23.889518	999.262629	14.861146
23.808097	993.635074	14.866163
23.729379	994.945583	14.871181
24.061379	1005.334425	14.876199
23.547623	1002.539581	14.881216
23.921022	1010.276040	14.886234
23.806973	1028.338350	14.891251
23.983024	1020.011347	14.896269
23.838635	1020.292579	14.901287
24.170109	1019.219064	14.906304
24.080218	1015.390791	14.911322
23.892116	1020.605632	14.916339
24.084672	1014.242251	14.921357
24.094558	1027.194565	14.926375
24.021309	1020.219208	14.931392
24.008487	1020.990680	14.936410
23.749692	1026.655665	14.941427
24.251911	1019.431224	14.946445
23.687270	1028.756600	14.951463
23.914827	1024.530061	14.956480
24.081663	1019.130311	14.961498
24.355527	1020.752669	14.966515
24.363265	1023.476103	14.971533
24.175629	1016.949993	14.976551
24.354922	1014.744595	14.981568
24.395975	1009.898157	14.986586
24.349780	1022.005273	14.991603
24.279075	1008.721783	14.996621
24.161246	1023.929696	15.001639
24.035443	1019.344245	15.006656
24.499425	1025.919548	15.011674
24.120419	1027.372333	15.016691
24.488105	1037.635959	15.021709
24.733955	1044.927172	15.026727
24.657030	1037.389257	15.031744
24.738126	1030.719607	15.036762
24.190678	1031.156358	15.041779
24.622160	1034.257369	15.046797
24.729016	1047.405018	15.051815
24.813453	1040.577531	15.056832
24.726908	1018.193593	15.061850
24.752688	1013.195436	15.066867
25.038934	1015.674677	15.071885
24.622998	1014.232739	15.076903
24.503784	1016.826984	15.081920
24.539963	1018.139619	15.086938
24.946822	1036.482221	15.091955
24.715635	1034.642732	15.096973
24.921864	1038.213818	15.101991
24.633235	1044.943773	15.107008
24.654803	1035.293336	15.112026
24.246875	1042.559835	15.117043
24.847223	1041.131980	15.122061
24.873661	1048.621781	15.127079
24.828507	1041.986420	15.132096
25.007162	1044.427771	15.137114
24.831883	1047.375451	15.142131
25.127756	1040.172900	15.147149
25.197210	1043.787825	15.152167
24.946171	1043.828094	15.157184
25.216283	1040.104416	15.162202
25.039925	1045.911988	15.167219
25.399759	1046.008981	15.172237
25.175050	1041.708281	15.177255
25.003702	1047.282250	15.182272
25.053033	1037.249863	15.187290
25.009589	1048.865786	15.192307
25.262713	1040.232327	15.197325
25.241511	1050.023166	15.202343
25.009559	1039.533853	15.207360
25.290616	1036.390441	15.212378
25.058921	1046.353274	15.217395
25.268097	1040.555085	15.222413
25.184307	1043.420534	15.227431
25.484188	1049.762475	15.232448
25.618424	1044.720268	15.237466
25.110201	1054.374858	15.242483
25.705501	1060.600475	15.247501
26.041641	1052.463423	15.252519
25.697353	1047.895506	15.257536
25.336413	1040.358843	15.262554
25.605550	1036.888575	15.267571
25.579224	1029.923032	15.272589
25.496363	1039.961221	15.277607
25.637440	1038.040336	15.282624
25.804687	1033.247695	15.287642
25.364817	1041.093433	15.292659
25.489015	1025.513717	15.297677
25.379757	1039.993554	15.302695
25.598746	1053.656572	15.307712
26.115221	1054.264977	15.312730
26.016975	1065.545166	15.317747
25.879375	1059.215547	15.322765
26.202083	1054.267544	15.327783
25.725652	1041.495467	15.332800
25.768492	1036.395482	15.337818
25.546267	1054.075534	15.342835
25.952300	1054.058195	15.347853
25.865528	1062.665590	15.352871
25.899328	1063.906250	15.357888
26.139097	1062.024677	15.362906
26.101525	1056.160445	15.367923
26.301003	1057.703438	15.372941
26.113410	1064.593463	15.377959
26.074298	1064.741502	15.382976
26.477003	1053.830061	15.387994
26.154698	1049.054147	15.393011
26.392109	1034.807576	15.398029
26.257434	1028.949404	15.403047
26.117196	1033.971001	15.408064
26.243631	1028.489603	15.413082
25.655933	1035.957800	15.418099
25.976924	1039.741815	15.423117
25.975884	1059.440939	15.428135
26.340472	1067.051421	15.433152
26.299958	1059.515552	15.438170
26.156935	1072.435667	15.443187
26.245494	1063.041939	15.448205
26.375761	1067.691646	15.453223
25.964090	1072.040830	15.458240
26.408072	1067.244938	15.463258
26.438305	1061.631009	15.468275
26.304033	1060.065492	15.473293
26.359237	1063.204501	15.478311
25.976723	1063.833594	15.483328
26.473514	1072.200059	15.488346
26.751114	1089.012359	15.493363
26.750712	1083.225558	15.498381
26.409447	1071.621090	15.503399
26.684301	1093.819808	15.508416
26.583949	1091.125750	15.513434
26.489902	1102.174065	15.518451
26.736596	1092.253307	15.523469
26.954758	1088.781719	15.528487
26.721264	1094.110790	15.533504
27.199243	1081.944646	15.538522
27.084828	1083.392988	15.543539
27.299179	1073.438076	15.548557
27.358219	1056.053471	15.553575
26.741693	1056.925950	15.558592
26.967039	1057.283491	15.563610
26.853909	1065.368135	15.568627
26.697392	1060.727794	15.573645
26.667829	1051.310442	15.578663
26.945324	1065.829293	15.583680
27.070119	1077.545819	15.588698
26.845399	1074.483067	15.593715
27.176105	1084.392406	15.598733
27.276055	1094.521025	15.603751
27.254457	1084.070488	15.608768
27.510937	1075.261870	15.613786
27.264723	1059.402999	15.618803
27.035441	1050.992764	15.623821
27.111736	1054.051330	15.628839
27.185881	1072.627939	15.633856
27.427689	1068.885173	15.638874
27.415857	1080.417429	15.643891
27.267563	1078.028318	15.648909
27.273587	1074.765171	15.653927
27.512563	1085.121718	15.658944
27.288528	1079.795298	15.663962
27.387491	1079.158406	15.668979
27.526509	1077.907945	15.673997
27.371142	1075.200643	15.679015
27.119366	1089.838538	15.684032
27.450263	1081.068384	15.689050
27.360202	1088.528023	15.694067
27.450448	1081.484089	15.699085
27.656418	1075.645499	15.704103
27.490650	1083.793604	15.709120
28.019230	1084.461428	15.714138
27.599053	1086.979419	15.719155
27.250441	1088.955893	15.724173
27.385710	1086.029203	15.729191
27.135363	1082.563127	15.734208
27.654067	1076.124107	15.739226
27.417926	1087.913938	15.744243
27.313829	1122.769794	15.749261
27.804241	1115.062702	15.754279
27.623598	1123.680386	15.759296
28.006415	1113.484648	15.764314
28.044909	1114.969953	15.769331
27.930566	1107.727403	15.774349
28.248475	1105.153821	15.779367
28.207334	1112.053544	15.784384
28.317878	1113.488032	15.789402
28.271937	1103.138890	15.794419
28.123938	1111.334512	15.799437
28.617789	1099.647164	15.804455
28.221007	1091.235306	15.809472
27.967568	1077.740227	15.814490
28.054870	1081.286248	15.819507
28.162796	1089.139023	15.824525
28.213853	1105.918263	15.829543
28.449608	1113.800999	15.834560
28.556468	1098.749356	15.839578
28.198138	1089.699017	15.844595
28.202646	1085.056581	15.849613
28.416420	1084.558679	15.854631
28.284423	1085.674775	15.859648
28.459685	1096.941253	15.864666
28.155581	1096.456735	15.869683
28.408162	1099.688540	15.874701
28.372492	1101.975322	15.879719
28.242874	1114.198066	15.884736
28.484380	1106.011584	15.889754
28.428034	1101.619519	15.894771
28.451224	1107.903371	15.899789
28.473672	1109.180452	15.904807
28.254701	1113.341612	15.909824
28.410779	1114.441652	15.914842
28.561463	1110.228922	15.919859
28.522065	1109.582637	15.924877
28.591201	1106.325147	15.929895
28.461371	1120.095771	15.934912
28.883410	1128.942949	15.939930
29.200049	1131.974209	15.944947
28.631702	1129.719724	15.949965
29.126283	1120.607265	15.954983
29.000746	1118.063508	15.960000
28.679552	1105.464815	15.965018
28.871959	1112.822787	15.970035
28.717870	1111.856597	15.975053
29.303269	1120.846027	15.980071
29.268895	1127.299515	15.985088
29.111656	1124.973171	15.990106
28.923917	1108.785598	15.995123
29.002705	1112.973201	16.000141
29.182928	1108.142286	16.005159
28.973233	1127.671862	16.010176
28.905899	1123.989399	16.015194
28.976527	1140.540617	16.020211
29.073684	1135.287217	16.025229
29.342380	1121.460284	16.030247
28.959608	1132.276248	16.035264
29.376519	1137.861821	16.040282
29.212046	1128.105716	16.045299
29.029208	1130.238225	16.050317
29.347918	1131.359518	16.055335
29.385519	1134.197758	16.060352
29.572080	1124.668811	16.065370
29.506338	1129.607774	16.070387
29.008440	1135.856771	16.075405
29.453295	1123.623517	16.080423
29.456975	1137.398032	16.085440
29.185058	1132.279002	16.090458
29.692281	1133.439442	16.095475
29.519060	1151.651340	16.100493
29.719967	1151.035939	16.105511
30.013826	1156.710358	16.110528
29.923493	1142.511234	16.115546
29.917503	1129.251918	16.120563
29.764621	1136.262282	16.125581
29.936943	1125.013156	16.130599
29.739388	1129.826852	16.135616
29.850095	1129.788976	16.140634
29.827239	1124.921232	16.145651
29.399831	1128.577671	16.150669
29.883836	1140.397405	16.155687
30.092445	1158.765490	16.160704
30.524056	1151.890445	16.165722
30.217054	1138.625646	16.170739
29.920380	1135.459527	16.175757
30.110721	1116.526512	16.180775
29.886789	1128.201172	16.185792
29.780242	1133.664165	16.190810
30.096297	1141.263552	16.195827
30.377753	1151.017198	16.200845
30.367555	1145.360922	16.205863
30.004542	1132.366183	16.210880
29.984650	1135.267075	16.215898
30.119108	1147.059194	16.220915
30.223001	1153.668393	16.225933
30.682177	1149.167352	16.230951
30.316402	1157.518855	16.235968
30.104731	1159.198219	16.240986
30.378652	1160.752946	16.246003
30.503741	1153.638925	16.251021
30.682879	1148.002787	16.256039
30.790532	1153.820160	16.261056
30.693755	1142.027204	16.266074
30.649186	1127.145974	16.271091
30.287727	1142.444778	16.276109
30.495074	1143.108783	16.281127
30.489939	1143.268707	16.286144
30.717082	1149.493307	16.291162
30.806223	1145.351730	16.296179
30.535776	1152.714331	16.301197
31.019964	1147.098753	16.306215
30.565643	1157.197841	16.311232
30.595170	1158.783680	16.316250
30.970999	1148.154880	16.321267
30.525098	1160.209458	16.326285
30.615180	1155.867955	16.331303
30.784169	1152.122625	16.336320
30.930789	1154.072031	16.341338
31.442950	1150.212195	16.346355
31.015877	1150.901880	16.351373
31.047528	1146.818235	16.356391
30.741859	1149.922011	16.361408
31.263863	1149.538540	16.366426
31.464897	1142.605894	16.371443
30.963298	1149.547613	16.376461
31.052372	1141.829012	16.381479
31.290662	1143.427172	16.386496
30.980446	1135.029795	16.391514
31.141347	1148.444194	16.396531
30.970801	1147.886463	16.401549
31.185346	1138.872138	16.406567
30.823434	1151.177579	16.411584
30.959058	1146.492190	16.416602
31.246219	1156.188302	16.421619
31.346228	1173.587446	16.426637
31.523077	1172.647121	16.431655
31.608310	1170.749282	16.436672
31.655171	1174.271889	16.441690
31.617035	1174.163371	16.446707
31.374176	1181.408330	16.451725
31.586282	1172.413249	16.456743
31.685105	1176.898121	16.461760
31.852738	1173.981982	16.466778
31.682218	1175.837255	16.471795
31.554095	1183.337620	16.476813
31.584195	1179.151967	16.481831
31.707853	1182.789742	16.486848
31.458991	1169.704405	16.491866
31.855893	1172.513662	16.496883
31.645743	1186.597606	16.501901
31.866795	1167.725693	16.506919
31.836306	1171.970067	16.511936
31.665021	1179.886298	16.516954
32.119842	1173.408661	16.521971
31.825471	1182.686309	16.526989
31.921314	1172.069113	16.532007
31.984927	1179.634851	16.537024
31.666618	1183.495698	16.542042
31.976267	1178.738499	16.547059
31.940402	1175.189429	16.552077
31.915695	1180.482086	16.557095
32.027058	1189.262447	16.562112
32.118898	1205.553954	16.567130
32.652882	1206.644066	16.572147
32.223243	1217.344871	16.577165
32.343713	1204.971378	16.582183
32.671764	1201.759089	16.587200
32.207540	1183.943408	16.592218
32.360674	1174.798857	16.597235
32.099231	1191.807361	16.602253
32.642189	1195.239839	16.607271
33.040604	1204.344088	16.612288
32.332249	1180.023584	16.617306
32.633210	1170.040636	16.622323
32.254022	1174.186468	16.627341
32.389777	1184.016858	16.632359
32.773683	1202.843104	16.637376
32.550433	1202.443213	16.642394
32.716665	1194.297002	16.647411
32.668744	1201.658744	16.652429
33.038594	1200.096179	16.657447
32.798739	1192.977423	16.662464
32.730013	1193.853775	16.667482
33.237823	1188.014192	16.672499
32.862565	1196.011727	16.677517
32.763020	1190.863611	16.682535
33.050235	1199.257284	16.687552
32.854524	1187.782090	16.692570
33.050529	1193.376176	16.697587
33.020662	1197.903601	16.702605
32.936885	1190.932986	16.707623
32.937883	1189.155546	16.712640
32.875752	1200.881535	16.717658
33.058780	1191.807711	16.722675
33.183332	1187.962494	16.727693
33.182783	1200.789213	16.732711
33.013230	1199.949751	16.737728
32.831826	1204.806513	16.742746
33.240587	1201.913259	16.747763
32.925212	1196.422039	16.752781
33.059710	1192.219732	16.757799
33.083556	1207.317152	16.762816
33.362438	1219.756404	16.767834
33.934832	1212.924944	16.772851
33.722873	1216.257606	16.777869
33.224907	1207.874401	16.782887
33.734623	1208.958945	16.787904
33.422028	1201.703922	16.792922
33.533357	1200.730000	16.797939
33.864120	1213.030411	16.802957
33.745562	1198.678431	16.807975
33.455492	1189.173550	16.812992
33.289105	1210.510022	16.818010
33.532551	1207.979759	16.823027
33.692848	1210.052834	16.828045
33.412327	1211.826555	16.833063
33.857876	1213.275263	16.838080
33.391980	1223.733318	16.843098
33.737569	1213.570190	16.848115
33.812968	1221.670470	16.853133
33.519490	1216.101817	16.858151
33.856935	1218.278774	16.863168
33.637655	1233.929376	16.868186
33.934929	1239.346881	16.873203
34.083798	1246.474338	16.878221
33.839963	1244.157066	16.883239
33.769497	1242.765397	16.888256
33.856783	1252.471429	16.893274
34.229214	1245.778812	16.898291
33.978301	1246.828943	16.903309
34.288320	1243.970305	16.908327
34.638217	1235.865564	16.913344
34.603803	1246.055044	16.918362
34.678361	1241.944080	16.923379
34.530279	1249.029238	16.928397
34.184225	1243.424915	16.933415
34.390205	1242.490950	16.938432
34.279153	1244.965957	16.943450
34.615010	1243.421394	16.948467
34.772933	1246.641588	16.953485
34.464516	1244.087651	16.958503
34.477802	1231.048537	16.963520
34.636949	1245.901049	16.968538
34.687154	1233.323234	16.973555
34.604656	1240.350736	16.978573
34.448945	1241.830848	16.983591
34.808838	1245.555231	16.988608
34.649400	1244.099101	16.993626
35.007408	1251.905786	16.998643
34.560661	1244.379555	17.003661
34.996066	1259.976107	17.008679
35.406438	1257.106181	17.013696
35.393700	1254.070929	17.018714
35.170974	1238.157779	17.023731
35.235806	1240.200467	17.028749
35.428293	1241.321451	17.033767
35.075621	1232.254388	17.038784
35.147001	1237.862076	17.043802
35.013830	1240.746450	17.048819
35.354650	1241.492993	17.053837
35.079211	1241.691309	17.058855
35.188465	1232.827426	17.063872
35.135787	1242.491281	17.068890
34.990944	1244.668083	17.073907
35.076993	1240.311467	17.078925
35.360298	1261.994718	17.083943
35.683793	1263.244248	17.088960
35.446824	1252.971083	17.093978
35.308832	1244.767971	17.098995
35.150971	1250.729976	17.104013
35.418511	1263.194670	17.109031
35.485113	1265.008989	17.114048
35.561142	1267.251242	17.119066
35.572332	1277.005607	17.124083
35.666971	1275.573445	17.129101
35.527088	1271.460493	17.134119
35.900066	1267.624398	17.139136
35.815101	1277.162864	17.144154
35.958660	1267.818434	17.149171
35.828838	1264.400731	17.154189
35.861976	1270.325990	17.159207
36.068847	1261.915283	17.164224
35.803439	1267.757594	17.169242
35.981196	1265.450157	17.174259
36.147964	1262.626948	17.179277
35.725155	1269.095259	17.184295
36.043512	1256.060950	17.189312
36.157113	1259.003498	17.194330
36.153445	1253.261195	17.199347
36.174446	1254.278969	17.204365
35.859535	1261.560627	17.209383
35.980696	1259.178847	17.214400
36.081183	1273.408387	17.219418
36.292800	1270.068362	17.224435
36.048959	1266.527271	17.229453
36.123178	1278.870226	17.234471
36.625678	1285.999506	17.239488
36.286740	1295.351973	17.244506
36.464175	1294.760760	17.249523
36.445271	1283.902234	17.254541
36.463626	1285.252342	17.259559
36.721360	1290.507857	17.264576
36.765868	1302.503213	17.269594
36.620493	1293.222152	17.274611
37.008295	1292.677612	17.279629
36.858566	1298.576991	17.284647
36.835927	1284.794796	17.289664
36.820584	1290.611391	17.294682
37.030541	1275.074359	17.299699
36.648599	1274.792585	17.304717
36.505100	1281.062198	17.309735
37.272517	1280.381609	17.314752
36.977322	1303.151340	17.319770
36.902857	1290.649987	17.324787
37.061499	1282.976846	17.329805
37.000211	1282.387526	17.334823
36.890236	1290.585050	17.339840
36.942965	1283.992169	17.344858
37.232102	1282.131009	17.349875
36.932876	1275.452691	17.354893
36.871849	1279.373204	17.359911
37.459250	1268.218216	17.364928
37.096436	1287.995798	17.369946
36.945993	1285.168120	17.374963
37.246477	1277.149888	17.379981
36.659242	1282.618815	17.384999
37.196642	1281.012217	17.390016
37.344276	1298.600545	17.395034
37.647119	1302.947524	17.400051
37.553459	1298.685620	17.405069
37.144836	1317.982909	17.410087
37.613732	1307.372185	17.415104
37.717538	1305.539008	17.420122
37.557451	1307.513756	17.425139
37.710084	1299.136847	17.430157
37.794649	1309.291665	17.435175
38.065470	1297.175687	17.440192
37.784563	1301.972845	17.445210
37.773427	1306.319564	17.450227
38.002947	1301.604993	17.455245
37.628065	1311.465000	17.460263
37.659645	1296.456620	17.465280
37.889983	1307.667287	17.470298
37.782211	1306.394820	17.475315
38.275580	1295.490763	17.480333
37.738845	1295.551427	17.485351
37.798393	1298.246200	17.490368
37.940227	1298.875044	17.495386
37.998717	1301.945941	17.500403
38.521948	1302.197778	17.505421
38.209996	1322.152912	17.510439
38.543453	1311.996370	17.515456
38.507746	1300.849500	17.520474
38.271637	1308.883106	17.525491
38.363163	1297.457969	17.530509
38.377789	1304.457428	17.535527
38.513754	1301.719348	17.540544
38.373464	1311.705536	17.545562
38.559172	1323.104233	17.550579
38.935037	1318.584968	17.555597
38.510076	1317.263986	17.560615
38.421128	1324.253232	17.565632
38.703627	1331.227285	17.570650
38.839963	1327.927568	17.575667
38.723572	1327.450855	17.580685
39.037469	1329.768439	17.585703
38.810503	1321.496103	17.590720
38.769906	1322.662133	17.595738
38.533351	1325.240540	17.600755
39.251525	1331.751850	17.605773
38.715642	1335.420920	17.610791
38.746293	1324.271314	17.615808
39.343265	1330.506224	17.620826
38.930682	1338.630913	17.625843
39.031650	1330.064023	17.630861
38.855011	1332.593549	17.635879
39.082325	1325.093479	17.640896
39.042131	1323.196749	17.645914
38.756750	1324.960246	17.650931
39.055318	1318.623871	17.655949
39.188974	1324.289300	17.660967
38.896653	1334.115706	17.665984
39.337122	1346.966600	17.671002
39.384684	1339.622606	17.676019
39.859081	1339.079984	17.681037
39.532651	1350.313415	17.686055
40.140985	1347.921564	17.691072
39.663994	1329.791557	17.696090
39.411960	1312.906145	17.701107
40.269361	1316.916145	17.706125
39.673507	1320.711180	17.711143
39.520869	1313.849015	17.716160
39.695303	1312.904348	17.721178
39.551631	1313.300300	17.726195
39.544894	1326.920927	17.731213
39.444574	1340.103457	17.736231
39.897525	1338.950772	17.741248
39.963097	1339.874927	17.746266
39.924461	1347.878634	17.751283
40.202063	1337.754577	17.756301
39.969848	1348.468036	17.761319
39.967414	1344.532918	17.766336
40.360049	1339.131645	17.771354
40.218677	1344.625440	17.776371
40.443983	1336.493324	17.781389
40.193176	1345.948172	17.786407
40.075787	1339.626217	17.791424
40.572987	1343.772324	17.796442
40.411594	1346.494478	17.801459
40.507612	1342.977816	17.806477
40.338297	1344.216288	17.811495
40.287734	1342.089973	17.816512
40.381193	1335.092594	17.821530
40.705826	1343.219260	17.826547
40.523925	1337.777483	17.831565
40.676077	1339.943112	17.836583
40.533841	1339.388724	17.841600
40.696456	1330.605934	17.846618
40.221936	1343.060056	17.851635
40.458023	1346.794774	17.856653
40.731039	1364.465432	17.861671
40.743285	1370.167547	17.866688
40.917144	1367.645209	17.871706
40.828679	1365.317295	17.876723
41.114078	1365.452907	17.881741
40.818369	1376.728649	17.886759
41.064438	1372.697261	17.891776
41.366176	1372.600604	17.896794
41.258410	1376.218708	17.901811
41.281028	1362.528322	17.906829
41.303622	1364.813719	17.911847
41.364898	1374.700163	17.916864
41.546976	1359.725917	17.921882
41.256495	1360.626634	17.926899
41.381366	1359.987172	17.931917
41.377622	1367.846897	17.936935
41.153569	1367.415668	17.941952
41.326348	1368.983404	17.946970
41.140151	1378.632464	17.951987
41.264086	1364.697826	17.957005
41.261056	1366.570455	17.962023
41.291863	1377.256144	17.967040
41.396403	1369.410686	17.972058
41.234891	1377.216927	17.977075
41.265298	1371.341725	17.982093
41.331306	1377.738416	17.987111
41.648787	1378.312509	17.992128
41.649762	1382.699792	17.997146
41.645167	1396.754301	18.002163
41.550946	1382.302303	18.007181
41.946096	1376.774772	18.012199
41.797542	1387.017162	18.017216
41.946205	1390.792576	18.022234
41.920152	1406.705132	18.027251
42.294746	1418.838278	18.032269
42.125493	1424.882396	18.037287
42.236459	1423.241547	18.042304
42.515589	1413.263488	18.047322
42.317687	1421.026790	18.052339
42.190314	1418.793163	18.057357
42.353589	1416.370034	18.062375
42.365938	1414.559295	18.067392
42.523982	1413.931843	18.072410
42.536695	1415.248256	18.077427
42.714400	1413.033615	18.082445
42.479990	1418.482500	18.087463
42.335150	1416.965820	18.092480
42.760996	1407.848416	18.097498
42.458832	1414.184290	18.102515
42.554985	1405.561495	18.107533
42.613503	1408.593083	18.112551
42.285362	1418.730428	18.117568
42.656304	1411.875950	18.122586
42.543343	1406.198208	18.127603
42.558556	1418.440580	18.132621
43.031184	1434.083296	18.137639
43.323620	1430.920684	18.142656
43.269301	1423.448176	18.147674
43.242251	1429.834563	18.152691
43.403342	1406.199286	18.157709
43.365315	1405.920860	18.162727
43.108083	1410.388658	18.167744
43.239104	1410.243722	18.172762
43.198880	1408.389457	18.177779
43.255520	1404.457486	18.182797
43.493791	1408.569402	18.187815
43.225815	1414.602519	18.192832
43.432032	1404.746207	18.197850
42.941223	1416.117590	18.202867
43.137987	1419.358370	18.207885
43.338204	1428.401562	18.212903
43.499050	1441.923209	18.217920
43.410923	1428.044355	18.222938
43.465327	1437.310584	18.227955
43.687946	1425.900619	18.232973
43.608051	1440.012798	18.237991
43.615361	1438.479715	18.243008
43.866639	1431.468132	18.248026
43.699446	1431.937053	18.253043
43.572482	1435.212163	18.258061
43.839552	1432.475172	18.263079
43.927707	1453.137467	18.268096
44.052129	1459.312516	18.273114
43.940906	1462.034555	18.278131
43.930167	1462.100993	18.283149
43.967295	1465.662977	18.288167
43.958845	1469.616054	18.293184
44.497118	1460.600239	18.298202
44.522835	1455.702615	18.303219
44.264206	1459.830871	18.308237
44.826206	1451.651285	18.313255
44.563293	1459.818239	18.318272
44.824798	1453.253333	18.323290
44.645641	1458.359934	18.328307
44.750738	1454.579099	18.333325
44.722649	1457.635522	18.338343
44.644577	1461.626443	18.343360
44.791725	1452.989194	18.348378
44.919117	1452.214044	18.353395
44.799168	1450.989124	18.358413
44.871465	1450.312425	18.363431
44.846354	1451.307679	18.368448
45.170357	1455.501892	18.373466
45.022995	1435.730402	18.378483
44.728678	1422.812534	18.383501
44.991784	1438.345523	18.388519
44.952143	1450.321388	18.393536
45.544369	1445.396340	18.398554
45.084690	1448.826764	18.403571
45.311675	1444.293452	18.408589
45.508099	1427.208966	18.413607
45.064917	1433.847341	18.418624
45.250267	1418.826894	18.423642
45.007625	1431.837148	18.428659
45.528941	1446.067383	18.433677
45.204852	1443.924901	18.438695
45.010172	1448.025651	18.443712
45.410176	1446.195555	18.448730
45.338042	1449.773388	18.453747
45.242064	1455.145152	18.458765
45.203413	1442.323346	18.463783
45.184620	1453.366218	18.468800
45.511748	1458.956800	18.473818
45.384973	1480.336114	18.478835
45.871603	1476.005206	18.483853
46.055077	1478.541820	18.488871
45.588935	1483.179812	18.493888
46.049749	1471.370022	18.498906
46.043827	1481.303435	18.503923
45.889681	1480.392284	18.508941
45.908193	1469.244503	18.513959
45.657601	1475.905665	18.518976
45.978921	1469.452337	18.523994
45.802625	1478.805723	18.529011
45.744409	1477.234322	18.534029
46.120610	1490.627286	18.539047
45.896598	1510.968209	18.544064
46.289126	1506.981068	18.549082
46.388702	1500.531630	18.554099
46.240547	1507.709734	18.559117
46.670243	1500.134825	18.564135
46.471264	1504.616956	18.569152
46.738165	1503.369661	18.574170
46.453753	1506.092587	18.579187
46.355006	1507.075994	18.584205
46.413309	1501.852254	18.589223
46.553779	1500.883104	18.594240
46.602079	1515.720538	18.599258
46.578765	1523.803696	18.604275
47.046442	1529.802907	18.609293
47.610217	1525.082148	18.614311
47.209085	1514.591154	18.619328
47.143367	1497.411538	18.624346
47.039457	1493.953467	18.629363
47.007100	1497.345639	18.634381
47.299035	1497.407851	18.639399
47.322632	1501.852911	18.644416
47.519531	1497.541463	18.649434
47.499675	1483.217504	18.654451
47.615290	1484.349196	18.659469
47.850328	1487.240963	18.664487
47.611968	1481.493526	18.669504
47.674535	1482.073672	18.674522
47.702283	1480.229007	18.679539
47.693252	1486.290070	18.684557
47.864458	1484.122073	18.689575
47.686325	1487.669628	18.694592
47.566296	1471.849954	18.699610
47.541834	1480.444513	18.704627
47.256187	1486.263396	18.709645
47.801413	1478.994121	18.714663
47.790243	1488.296010	18.719680
47.837675	1470.115223	18.724698
47.739202	1487.848426	18.729715
47.512404	1487.881681	18.734733
48.420700	1493.332397	18.739751
47.990802	1508.030581	18.744768
47.894122	1509.559508	18.749786
48.111332	1501.450613	18.754803
47.982045	1519.275286	18.759821
48.145107	1511.055471	18.764839
47.993640	1513.437865	18.769856
48.104177	1516.133985	18.774874
48.272562	1508.430857	18.779891
48.009695	1517.744591	18.784909
48.474759	1503.185971	18.789927
48.363800	1518.991067	18.794944
48.419884	1523.261062	18.799962
48.574601	1539.947193	18.804979
48.594530	1552.402863	18.809997
48.983262	1550.500618	18.815015
48.945258	1546.506623	18.820032
48.969873	1542.052748	18.825050
49.092490	1543.614345	18.830067
48.760432	1552.305194	18.835085
48.972999	1542.650701	18.840103
49.014181	1553.559813	18.845120
48.966361	1542.367497	18.850138
49.080320	1541.105264	18.855155
48.891815	1549.331188	18.860173
49.184072	1541.554803	18.865191
48.982658	1542.362672	18.870208
49.069714	1546.302112	18.875226
49.225187	1539.771382	18.880243
49.093139	1548.290328	18.885261
49.182907	1534.633116	18.890279
49.451523	1540.605876	18.895296
49.142153	1543.123572	18.900314
49.718791	1549.582051	18.905331
49.662772	1572.883505	18.910349
49.899188	1563.881161	18.915367
50.014132	1551.317914	18.920384
49.905664	1542.502724	18.925402
49.920049	1527.798873	18.930419
49.653341	1531.890685	18.935437
49.623244	1536.761178	18.940455
49.524547	1554.831133	18.945472
49.479924	1570.676043	18.950490
49.552367	1561.196472	18.955507
49.780255	1560.211803	18.960525
50.172410	1556.806741	18.965543
49.918023	1569.207070	18.970560
50.245146	1556.429078	18.975578
50.307709	1568.052106	18.980595
50.119038	1580.204432	18.985613
50.568190	1578.729859	18.990631
50.520223	1581.246772	18.995648
50.721448	1585.101946	19.000666
50.394780	1563.549857	19.005683
50.544276	1566.077748	19.010701
50.495573	1557.448076	19.015719
50.785268	1581.760944	19.020736
50.966834	1566.355548	19.025754
50.525351	1563.033097	19.030771
50.450575	1564.478310	19.035789
51.072391	1573.614808	19.040807
51.103141	1584.391897	19.045824
51.139396	1578.241966	19.050842
51.076277	1563.251559	19.055859
50.776751	1549.621811	19.060877
51.060308	1566.070343	19.065895
51.111023	1573.572275	19.070912
51.359365	1582.065183	19.075930
51.364053	1575.923434	19.080947
51.319894	1581.253946	19.085965
51.489626	1582.551625	19.090983
51.313422	1558.645842	19.096000
51.096385	1575.762545	19.101018
51.271897	1569.529060	19.106035
50.942477	1585.252662	19.111053
51.193385	1571.464321	19.116071
51.132577	1594.662752	19.121088
51.290804	1590.094743	19.126106
51.364933	1591.550818	19.131123
51.222330	1600.118670	19.136141
51.741179	1610.766024	19.141159
52.035777	1603.130808	19.146176
51.816278	1606.809261	19.151194
52.338532	1602.491513	19.156211
52.133385	1612.626680	19.161229
52.564804	1602.470044	19.166247
52.018686	1608.077252	19.171264
52.087990	1611.940888	19.176282
52.485819	1597.496720	19.181299
52.174275	1613.107386	19.186317
52.462309	1604.383083	19.191335
52.537901	1599.944656	19.196352
52.389062	1605.696149	19.201370
52.467878	1602.504647	19.206387
52.215227	1603.684069	19.211405
52.470645	1603.912558	19.216423
52.364087	1599.555092	19.221440
52.445693	1606.852336	19.226458
52.390341	1597.257839	19.231475
52.495470	1606.926657	19.236493
52.541823	1594.062845	19.241511
52.813285	1620.258496	19.246528
52.959590	1617.814445	19.251546
53.210566	1627.227203	19.256563
53.016731	1632.484074	19.261581
52.751519	1639.205846	19.266599
53.071191	1635.274336	19.271616
53.173637	1641.651175	19.276634
53.365873	1630.928607	19.281651
52.919422	1636.348467	19.286669
52.961969	1623.120285	19.291687
53.116040	1617.494256	19.296704
53.228930	1621.536565	19.301722
53.309701	1623.966885	19.306739
53.417642	1618.340348	19.311757
53.487042	1614.700448	19.316775
53.355154	1629.102681	19.321792
53.050859	1626.368686	19.326810
53.470125	1624.820223	19.331827
53.468777	1654.800196	19.336845
53.513284	1644.733552	19.341863
53.890982	1657.118096	19.346880
53.748479	1654.493576	19.351898
53.946728	1654.281286	19.356915
53.622980	1649.138874	19.361933
53.781822	1648.547467	19.366951
54.060699	1642.665564	19.371968
53.684391	1648.489532	19.376986
54.061063	1657.523603	19.382003
54.235979	1671.820318	19.387021
54.233898	1673.480471	19.392039
54.676758	1668.071069	19.397056
54.700723	1664.603576	19.402074
54.820854	1662.582129	19.407091
54.985755	1668.753959	19.412109
54.976914	1641.417223	19.417127
54.900273	1637.100593	19.422144
54.639877	1637.744836	19.427162
54.905642	1627.207178	19.432179
54.803140	1636.322375	19.437197
54.740425	1634.205820	19.442215
55.223851	1628.648387	19.447232
54.831535	1623.158260	19.452250
55.021190	1616.349903	19.457267
54.857290	1636.333767	19.462285
55.127021	1627.145168	19.467303
55.077881	1627.758866	19.472320
54.681162	1630.167808	19.477338
55.151226	1636.272080	19.482355
55.237086	1653.065280	19.487373
54.852231	1665.702009	19.492391
55.310458	1657.859767	19.497408
55.106947	1667.961677	19.502426
55.432620	1663.530539	19.507443
55.049935	1672.879212	19.512461
55.252792	1670.592879	19.517479
55.963897	1685.497820	19.522496
55.524150	1693.009604	19.527514
55.926797	1683.544149	19.532531
55.895303	1695.433970	19.537549
55.711563	1690.294383	19.542567
56.229028	1689.576566	19.547584
55.914602	1687.469471	19.552602
56.177477	1683.766451	19.557619
55.865141	1685.848902	19.562637
56.198941	1691.180528	19.567655
56.344659	1681.048952	19.572672
56.093168	1687.816536	19.577690
56.673569	1678.809601	19.582707
56.483742	1681.664556	19.587725
55.885065	1682.270725	19.592743
56.438656	1691.809089	19.597760
56.086376	1683.289106	19.602778
56.469936	1685.576764	19.607795
56.459473	1685.222361	19.612813
56.210640	1683.059187	19.617831
56.507783	1674.034506	19.622848
56.410390	1688.895353	19.627866
56.724936	1705.007183	19.632883
56.948427	1718.060547	19.637901
56.783036	1717.000158	19.642919
57.128405	1718.295008	19.647936
57.096134	1712.968443	19.652954
57.015671	1707.082472	19.657971
56.914301	1721.837805	19.662989
56.883235	1713.459279	19.668007
56.981257	1710.602902	19.673024
56.910240	1714.931764	19.678042
56.952504	1700.906007	19.683059
57.441690	1720.969882	19.688077
57.615404	1726.056482	19.693095
57.880343	1725.363992	19.698112
57.646523	1732.331705	19.703130
58.063096	1726.300390	19.708147
57.825963	1718.666542	19.713165
57.533785	1701.238073	19.718183
58.104608	1701.847286	19.723200
57.870004	1708.776573	19.728218
57.894250	1695.073815	19.733235
57.872373	1703.428200	19.738253
58.080074	1713.430740	19.743271
58.286744	1709.052389	19.748288
58.037499	1711.186919	19.753306
58.101662	1715.486358	19.758323
58.316638	1718.144624	19.763341
58.200242	1722.555447	19.768359
58.337604	1710.372318	19.773376
58.080435	1717.154192	19.778394
57.974018	1713.803437	19.783411
58.071270	1709.661194	19.788429
58.252573	1713.061028	19.793447
58.692581	1724.256673	19.798464
58.449584	1741.447712	19.803482
58.751381	1749.905452	19.808499
58.899783	1745.521439	19.813517
58.562853	1748.068733	19.818535
59.192852	1736.281301	19.823552
58.971531	1747.606815	19.828570
59.008696	1741.308015	19.833587
59.251131	1739.153004	19.838605
59.007970	1744.328903	19.843623
59.234071	1742.397514	19.848640
59.079802	1740.422177	19.853658
59.171106	1741.615971	19.858675
59.121468	1744.206326	19.863693
58.524047	1739.212922	19.868711
59.272363	1743.137411	19.873728
59.283432	1765.341477	19.878746
59.257927	1773.063315	19.883763
59.399235	1761.033677	19.888781
59.353816	1773.174330	19.893799
59.419086	1767.212395	19.898816
59.553422	1774.331421	19.903834
59.714798	1777.269602	19.908851
59.900284	1780.466645	19.913869
59.924115	1791.919843	19.918887
60.433878	1797.991111	19.923904
60.267482	1793.541665	19.928922
60.216230	1792.446550	19.933939
60.613212	1800.168667	19.938957
60.518277	1785.548846	19.943975
60.478397	1765.997299	19.948992
60.268054	1759.460315	19.954010
60.345680	1758.079585	19.959027
60.558811	1773.349549	19.964045
60.676380	1787.479339	19.969063
60.961327	1779.779502	19.974080
60.632849	1768.288052	19.979098
60.489921	1765.069741	19.984115
60.720930	1770.420149	19.989133
60.640550	1788.932655	19.994151
60.850530	1781.998280	19.999168
60.688735	1800.007812	20.004186
60.904088	1795.970197	20.009203
61.094653	1787.795391	20.014221
60.891612	1787.363156	20.019239
61.107428	1782.623875	20.024256
61.130159	1792.063703	20.029274
60.958495	1788.237253	20.034291
61.318887	1791.312806	20.039309
61.140280	1805.363214	20.044327
61.638159	1801.242786	20.049344
61.508279	1811.363728	20.054362
61.549209	1807.945406	20.059379
61.753712	1810.538503	20.064397
61.415907	1814.401049	20.069415
61.646642	1809.133182	20.074432
62.061922	1806.306418	20.079450
61.660527	1805.958514	20.084467
61.986197	1806.460533	20.089485
62.132113	1799.716484	20.094503
62.202151	1795.118429	20.099520
62.033151	1795.836982	20.104538
62.331415	1796.169545	20.109555
62.554765	1788.603014	20.114573
62.313273	1803.505049	20.119591
62.557947	1779.571108	20.124608
62.277324	1793.671595	20.129626
62.296151	1786.953326	20.134643
62.726785	1784.166591	20.139661
62.811349	1798.027939	20.144679
62.668910	1786.707373	20.149696
63.012360	1798.291296	20.154714
62.855726	1792.535419	20.159731
62.811836	1785.188481	20.164749
62.707035	1786.741541	20.169767
62.675500	1785.203605	20.174784
63.060014	1795.884319	20.179802
62.819963	1808.601115	20.184819
62.710847	1819.145057	20.189837
62.808157	1818.598852	20.194855
63.287843	1811.394926	20.199872
63.195442	1821.137862	20.204890
63.010319	1813.172400	20.209907
63.393486	1814.860009	20.214925
63.475315	1829.186670	20.219943
63.457255	1814.589168	20.224960
63.449294	1828.838122	20.229978
63.745611	1838.257945	20.234995
63.881135	1849.715401	20.240013
63.936018	1849.684068	20.245031
63.692579	1839.324996	20.250048
63.746495	1853.022963	20.255066
63.760798	1845.801999	20.260083
63.994907	1850.142805	20.265101
64.024430	1844.387895	20.270119
63.935087	1837.234590	20.275136
63.836794	1843.641959	20.280154
63.822919	1852.135158	20.285171
64.122118	1852.285096	20.290189
64.291303	1869.151778	20.295207
64.176998	1866.708347	20.300224
64.361940	1863.381882	20.305242
64.561227	1867.751843	20.310259
64.900262	1866.411215	20.315277
64.589290	1868.848206	20.320295
64.665834	1864.204258	20.325312
65.128039	1865.100589	20.330330
64.955461	1862.650721	20.335347
64.822341	1865.412507	20.340365
64.534210	1877.392171	20.345383
64.915900	1882.551056	20.350400
65.122139	1891.105920	20.355418
65.667265	1892.681190	20.360435
65.590082	1881.818139	20.365453
65.301766	1890.395240	20.370471
65.450419	1884.416027	20.375488
65.970600	1885.771109	20.380506
65.720743	1883.905382	20.385523
66.011576	1877.115377	20.390541
65.731245	1883.403137	20.395559
65.828954	1857.729066	20.400576
65.760300	1856.018496	20.405594
65.389489	1869.404311	20.410611
65.938279	1870.336387	20.415629
66.020615	1876.539564	20.420647
65.866336	1884.378742	20.425664
65.876644	1886.889561	20.430682
65.943699	1878.228652	20.435699
66.071621	1881.585914	20.440717
65.888012	1895.847215	20.445735
66.010214	1882.116862	20.450752
66.088002	1895.211713	20.455770
66.152681	1904.866731	20.460787
66.670459	1904.962148	20.465805
66.727280	1908.128612	20.470823
66.667737	1911.007667	20.475840
66.831830	1901.256844	20.480858
66.727626	1914.165222	20.485875
66.725886	1906.723406	20.490893
66.872300	1916.401578	20.495911
66.887333	1908.075366	20.500928
66.838902	1907.606671	20.505946
66.917543	1919.409109	20.510963
67.009101	1910.415497	20.515981
67.449126	1926.534306	20.520999
67.804153	1932.859195	20.526016
67.644650	1914.271959	20.531034
67.364955	1917.140504	20.536051
67.479272	1910.452570	20.541069
67.480812	1922.570127	20.546087
67.462608	1924.132201	20.551104
67.704741	1929.815965	20.556122
67.376843	1946.851677	20.561139
67.809533	1934.843071	20.566157
67.601208	1941.172857	20.571175
67.482096	1937.424508	20.576192
67.831603	1938.622761	20.581210
67.845997	1955.791881	20.586227
67.926092	1964.166335	20.591245
67.972236	1963.887846	20.596263
68.129403	1960.955131	20.601280
68.345875	1960.146086	20.606298
67.997964	1967.031426	20.611315
68.246452	1959.409672	20.616333
68.178350	1972.801579	20.621351
68.779705	1983.633479	20.626368
68.888791	1982.421539	20.631386
68.909277	1980.548867	20.636403
68.928339	1983.286406	20.641421
69.071783	1986.431208	20.646439
69.130674	1981.557219	20.651456
69.214451	1974.542987	20.656474
69.023206	1980.746578	20.661491
69.348433	1977.042193	20.666509
69.184610	1966.222785	20.671527
69.165662	1970.139132	20.676544
69.531219	1967.875573	20.681562
69.596203	1975.844223	20.686579
69.430040	1973.476687	20.691597
69.434129	1976.826977	20.696615
69.788313	1970.946306	20.701632
69.868390	1962.181019	20.706650
69.494799	1983.441550	20.711667
69.907419	1972.418518	20.716685
69.953844	1968.036543	20.721703
69.634564	1972.007078	20.726720
69.785297	1970.241058	20.731738
69.469879	1983.076209	20.736755
69.995608	1969.919314	20.741773
69.853892	1979.564823	20.746791
70.156519	1995.390213	20.751808
70.190550	2002.428602	20.756826
70.031405	2004.143729	20.761843
70.306208	2000.806049	20.766861
70.326500	2007.812809	20.771879
70.418737	2007.603265	20.776896
70.514355	1996.139959	20.781914
70.543790	2010.141655	20.786931
70.717600	2018.789074	20.791949
70.856381	2030.228062	20.796967
70.811601	2035.263881	20.801984
71.220631	2029.685129	20.807002
71.064801	2030.055508	20.812019
70.986329	2027.272049	20.817037
71.137484	2028.546776	20.822055
71.132402	2028.623326	20.827072
71.351596	2024.922468	20.832090
71.036630	2023.577579	20.837107
71.395146	2017.272246	20.842125
71.553502	2034.620646	20.847143
71.520335	2039.229874	20.852160
71.741403	2043.728557	20.857178
71.567471	2060.485790	20.862195
72.130562	2047.146680	20.867213
72.012070	2047.357726	20.872231
71.950766	2055.353638	20.877248
71.975436	2048.367674	20.882266
72.016548	2045.905720	20.887283
72.076129	2046.120617	20.892301
72.018675	2044.604091	20.897319
72.059814	2047.005408	20.902336
72.609360	2043.153544	20.907354
72.239827	2059.481047	20.912371
72.456152	2060.131083	20.917389
72.765023	2056.691998	20.922407
72.690603	2063.711530	20.927424
72.897438	2062.797831	20.932442
72.940462	2063.569892	20.937459
73.173101	2057.898916	20.942477
73.088431	2058.371998	20.947495
72.913837	2058.961673	20.952512
73.279779	2056.130146	20.957530
72.776723	2061.364906	20.962547
73.096666	2055.867996	20.967565
73.152064	2058.742121	20.972583
72.843944	2059.283086	20.977600
72.971889	2056.482435	20.982618
73.092302	2070.000893	20.987635
73.261933	2080.079762	20.992653
73.298923	2091.221981	20.997671
73.200263	2098.174605	21.002688
73.781081	2089.872899	21.007706
73.633033	2093.164102	21.012723
73.616614	2094.473424	21.017741
74.167231	2100.046709	21.022759
74.095533	2110.297800	21.027776
74.391837	2109.962897	21.032794
74.224078	2118.590123	21.037811
74.381745	2114.909279	21.042829
74.474168	2110.744096	21.047847
74.404328	2115.727307	21.052864
74.670384	2103.581532	21.057882
74.256588	2112.152031	21.062899
74.446239	2112.748905	21.067917
74.520528	2106.624935	21.072935
74.246467	2110.744821	21.077952
74.804791	2120.589476	21.082970
75.020413	2137.027468	21.087987
75.574091	2130.612308	21.093005
75.156444	2129.071412	21.098023
74.882121	2144.624009	21.103040
75.496190	2137.464566	21.108058
75.419039	2138.807961	21.113075
75.420807	2146.901624	21.118093
75.340596	2143.069147	21.123111
75.244186	2144.158408	21.128128
75.346696	2132.067794	21.133146
75.222813	2139.214808	21.138163
75.358035	2130.299045	21.143181
75.395744	2139.125552	21.148199
75.728496	2157.157338	21.153216
76.120867	2151.088024	21.158234
76.164732	2154.267620	21.163251
76.227662	2162.900558	21.168269
76.307166	2151.329582	21.173287
76.275455	2159.863559	21.178304
76.664333	2156.635076	21.183322
76.509766	2153.855075	21.188339
76.631613	2155.394053	21.193357
76.818358	2157.945999	21.198375
76.579006	2159.754950	21.203392
76.761404	2150.495790	21.208410
76.661483	2153.224019	21.213427
76.530352	2160.312420	21.218445
76.834180	2147.359079	21.223463
76.530949	2152.742913	21.228480
76.715951	2145.671555	21.233498
77.034461	2160.757586	21.238515
77.098915	2180.574423	21.243533
77.634577	2178.167296	21.248551
77.444421	2182.701711	21.253568
77.501028	2176.388611	21.258586
77.735929	2174.661057	21.263603
77.595353	2170.302550	21.268621
77.655232	2173.748602	21.273639
77.708353	2173.943294	21.278656
78.029700	2171.244708	21.283674
77.933753	2172.854601	21.288691
77.734370	2174.199401	21.293709
77.791678	2171.728551	21.298727
77.919649	2171.349700	21.303744
78.007961	2168.509728	21.308762
77.894770	2166.811729	21.313779
77.877301	2191.787338	21.318797
78.625119	2207.670176	21.323815
78.222497	2206.652300	21.328832
78.667570	2198.009575	21.333850
78.599451	2205.288523	21.338867
78.303476	2198.446435	21.343885
78.764418	2197.649519	21.348903
78.793520	2198.668428	21.353920
78.858315	2198.346846	21.358938
79.191973	2195.396165	21.363955
78.702207	2204.988781	21.368973
79.193783	2219.102609	21.373991
79.369321	2238.640671	21.379008
79.189005	2231.942943	21.384026
79.549841	2231.967433	21.389043
79.333018	2230.296178	21.394061
79.675982	2230.417120	21.399079
79.646970	2232.408842	21.404096
79.753321	2226.768167	21.409114
79.859719	2223.509206	21.414131
79.604439	2229.819074	21.419149
79.986568	2223.340776	21.424167
79.966897	2220.989953	21.429184
79.984982	2210.492947	21.434202
80.218723	2230.153073	21.439219
80.106619	2235.391619	21.444237
80.812023	2240.742061	21.449255
80.517619	2242.549576	21.454272
80.718749	2245.391846	21.459290
80.862345	2237.287206	21.464307
80.528894	2239.384898	21.469325
80.550335	2233.615392	21.474343
80.758186	2242.218974	21.479360
80.942075	2234.389501	21.484378
80.925716	2236.831481	21.489395
81.077190	2233.962546	21.494413
81.401009	2237.341352	21.499431
80.969578	2249.297764	21.504448
81.124478	2241.236940	21.509466
81.389456	2236.875878	21.514483
81.180554	2233.011200	21.519501
81.247445	2236.873028	21.524519
81.171376	2240.251893	21.529536
81.213274	2235.375809	21.534554
81.333933	2257.118741	21.539571
81.252697	2270.778089	21.544589
81.567173	2261.331830	21.549607
81.252481	2273.025809	21.554624
81.620296	2298.053425	21.559642
81.711262	2293.648518	21.564659
81.771064	2297.214170	21.569677
82.269356	2288.905849	21.574695
82.072361	2301.338547	21.579712
82.030593	2309.163944	21.584730
82.379427	2315.121089	21.589747
82.519325	2323.660045	21.594765
82.626403	2329.187739	21.599783
82.641337	2327.144436	21.604800
82.976015	2325.114641	21.609818
83.158627	2321.677539	21.614835
82.782713	2319.419692	21.619853
83.269073	2319.382477	21.624871
82.999631	2317.703872	21.629888
83.195901	2311.970954	21.634906
83.595554	2313.298894	21.639923
83.240340	2323.829745	21.644941
83.769393	2325.340774	21.649959
83.801981	2341.930892	21.654976
83.846416	2339.345654	21.659994
84.047765	2330.825095	21.665011
83.453578	2330.570842	21.670029
83.952772	2331.942690	21.675047
84.373347	2337.143521	21.680064
84.155090	2336.406930	21.685082
84.749568	2335.690967	21.690099
84.339413	2328.886690	21.695117
84.586418	2316.196324	21.700135
84.195029	2312.849186	21.705152
84.185067	2312.958764	21.710170
84.277977	2327.689234	21.715187
84.646746	2326.753630	21.720205
84.739361	2333.345503	21.725223
84.719761	2337.019789	21.730240
84.700280	2331.926929	21.735258
85.087571	2327.460599	21.740275
84.858183	2333.773462	21.745293
85.110717	2328.654529	21.750311
84.876056	2327.012064	21.755328
84.950166	2351.830188	21.760346
85.160643	2347.879724	21.765363
84.979561	2357.047230	21.770381
85.712392	2346.638296	21.775399
85.304399	2358.631174	21.780416
85.373577	2357.805483	21.785434
85.502621	2350.904984	21.790451
85.483085	2370.426351	21.795469
85.932141	2370.504419	21.800487
86.128695	2380.292105	21.805504
85.835205	2385.602892	21.810522
86.156423	2380.675138	21.815539
86.066804	2372.689418	21.820557
86.277327	2368.671295	21.825575
85.923104	2374.011427	21.830592
86.534029	2388.863860	21.835610
86.656902	2397.448837	21.840627
86.393638	2409.703417	21.845645
86.528605	2408.549455	21.850663
86.882047	2398.955311	21.855680
86.945048	2407.490061	21.860698
87.375857	2394.745146	21.865715
87.123971	2409.384380	21.870733
87.185475	2407.921997	21.875751
87.112766	2404.976298	21.880768
87.329536	2412.348356	21.885786
87.655537	2405.085274	21.890803
87.162653	2409.544543	21.895821
87.338958	2414.444555	21.900839
87.776666	2414.554324	21.905856
87.612756	2428.363081	21.910874
87.803369	2428.756879	21.915891
87.558644	2426.411235	21.920909
88.157864	2422.213913	21.925927
88.120318	2419.959511	21.930944
88.202660	2423.722176	21.935962
88.072750	2419.131426	21.940979
88.033104	2443.365329	21.945997
88.248097	2449.750534	21.951015
88.274161	2450.469473	21.956032
88.367933	2460.220116	21.961050
88.349483	2451.109995	21.966067
88.337300	2459.490797	21.971085
88.693940	2474.497137	21.976103
88.822262	2479.733613	21.981120
88.817380	2481.959068	21.986138
89.305704	2465.486759	21.991155
89.230657	2475.895170	21.996173
89.109248	2476.821687	22.001191
89.281294	2473.460172	22.006208
89.475225	2489.684142	22.011226
89.974120	2493.996291	22.016243
90.124276	2499.270981	22.021261
90.318815	2485.136808	22.026279
90.193212	2480.151276	22.031296
89.528834	2469.680323	22.036314
89.536052	2457.252248	22.041331
89.811329	2479.014117	22.046349
89.924713	2487.261644	22.051367
90.551028	2494.769799	22.056384
90.267374	2491.296890	22.061402
90.321025	2491.923335	22.066419
90.544227	2487.103206	22.071437
90.545012	2496.687002	22.076455
90.335571	2488.708527	22.081472
90.193547	2493.883504	22.086490
91.074608	2509.151561	22.091507
90.790211	2517.842456	22.096525
90.705884	2517.778262	22.101543
90.928373	2522.626111	22.106560
91.045036	2514.867776	22.111578
91.404659	2522.912447	22.116595
91.373990	2522.503040	22.121613
91.472213	2534.098343	22.126631
91.704406	2548.776936	22.131648
91.774820	2555.896315	22.136666
91.966850	2545.567189	22.141683
91.882925	2538.760343	22.146701
91.969586	2549.474957	22.151719
91.869428	2542.731265	22.156736
92.114565	2548.839550	22.161754
92.200622	2539.615958	22.166771
92.370819	2542.742458	22.171789
92.273068	2534.805140	22.176807
92.263366	2539.424943	22.181824
92.109796	2544.918772	22.186842
92.588558	2555.218474	22.191859
92.269424	2557.658449	22.196877
92.418321	2572.205617	22.201895
92.295197	2575.725782	22.206912
92.430603	2592.314735	22.211930
92.840291	2587.066823	22.216947
93.068840	2595.004223	22.221965
92.997142	2600.336353	22.226983
93.164507	2596.714410	22.232000
93.116454	2620.191679	22.237018
93.973653	2613.992991	22.242035
94.149698	2613.168336	22.247053
93.867458	2616.127091	22.252071
94.436103	2606.780092	22.257088
94.362519	2607.608533	22.262106
94.400608	2609.735911	22.267123
93.945464	2603.586038	22.272141
94.440058	2600.947846	22.277159
94.538355	2605.074564	22.282176
94.328036	2608.230293	22.287194
94.632235	2611.947403	22.292211
94.519957	2610.071437	22.297229
94.515818	2613.622192	22.302247
94.922604	2605.421105	22.307264
94.801047	2605.337677	22.312282
94.946104	2603.627548	22.317299
94.781580	2602.408062	22.322317
94.847135	2600.945800	22.327335
95.059148	2603.276699	22.332352
94.568870	2613.558709	22.337370
94.954937	2613.444674	22.342387
95.096364	2627.046824	22.347405
95.062676	2641.024583	22.352423
95.416847	2647.533201	22.357440
95.559228	2658.465548	22.362458
95.725479	2658.990666	22.367475
95.388738	2667.244000	22.372493
95.869620	2664.536405	22.377511
96.063986	2665.396060	22.382528
96.189101	2688.996850	22.387546
96.320097	2682.833706	22.392563
96.259860	2692.877292	22.397581
96.321069	2690.640923	22.402599
96.564638	2685.643645	22.407616
96.557602	2692.357762	22.412634
96.670577	2681.607735	22.417651
96.878487	2691.388314	22.422669
96.917080	2691.525550	22.427687
97.334813	2693.735561	22.432704
97.159618	2713.585046	22.437722
97.586560	2712.882414	22.442739
97.500703	2705.317524	22.447757
97.698752	2701.827530	22.452775
97.523230	2706.226052	22.457792
97.519085	2712.238864	22.462810
97.966609	2697.526902	22.467827
97.673270	2703.796633	22.472845
97.551462	2704.090021	22.477863
98.046038	2695.365173	22.482880
97.873282	2699.252754	22.487898
97.988498	2697.374323	22.492915
98.127152	2721.318321	22.497933
98.464184	2726.822083	22.502951
98.396844	2721.865719	22.507968
98.684536	2723.620583	22.512986
98.844627	2721.218203	22.518003
98.839689	2711.260177	22.523021
98.592825	2728.069921	22.528039
99.075359	2711.838172	22.533056
98.465001	2738.436823	22.538074
98.819994	2746.166934	22.543091
99.062785	2748.489016	22.548109
99.094678	2752.646815	22.553127
99.312493	2742.518740	22.558144
99.677374	2767.164563	22.563162
100.034050	2762.536228	22.568179
100.094422	2760.344818	22.573197
99.750053	2756.831970	22.578215
100.120527	2744.792510	22.583232
100.381197	2766.642091	22.588250
99.925954	2771.650799	22.593267
100.364251	2775.837404	22.598285
100.215599	2771.411569	22.603303
100.431803	2772.313371	22.608320
100.184129	2773.173515	22.613338
100.359461	2769.761854	22.618355
100.458695	2768.795267	22.623373
100.181365	2767.974466	22.628391
100.722611	2775.648149	22.633408
100.693115	2782.044957	22.638426
100.785208	2785.764472	22.643443
101.287999	2776.880161	22.648461
101.013324	2776.939923	22.653479
101.114749	2784.921298	22.658496
101.457847	2814.365763	22.663514
101.881150	2808.158314	22.668531
101.770576	2804.916519	22.673549
101.545687	2809.277321	22.678567
102.223102	2805.687264	22.683584
101.992456	2813.863194	22.688602
101.814862	2805.445263	22.693619
102.287950	2812.129283	22.698637
101.915456	2808.286603	22.703655
102.188423	2822.549940	22.708672
102.195043	2835.560235	22.713690
102.713466	2832.439167	22.718707
102.860570	2833.775182	22.723725
102.748344	2842.848632	22.728743
102.920318	2842.077316	22.733760
102.955394	2840.186476	22.738778
102.735802	2838.971817	22.743795
102.929762	2850.275223	22.748813
103.103343	2867.921885	22.753831
103.241494	2860.742811	22.758848
103.517183	2867.205836	22.763866
103.370672	2868.118287	22.768883
103.747823	2864.377087	22.773901
103.406606	2881.835266	22.778919
104.074971	2879.704993	22.783936
103.791224	2894.728146	22.788954
104.163638	2895.713598	22.793971
104.270084	2885.050989	22.798989
104.364128	2890.726497	22.804007
104.534688	2888.418385	22.809024
104.636133	2875.520274	22.814042
104.574973	2882.050391	22.819059
104.670907	2875.048735	22.824077
104.528643	2898.963879	22.829095
104.895960	2908.902464	22.834112
104.772823	2914.878485	22.839130
104.982644	2920.555995	22.844147
105.266058	2915.321025	22.849165
105.122093	2920.958984	22.854183
105.443997	2902.794784	22.859200
105.552203	2918.908619	22.864218
105.539615	2941.395135	22.869235
105.782369	2932.750421	22.874253
105.258450	2939.967120	22.879271
105.702493	2941.608980	22.884288
105.989697	2939.221692	22.889306
106.014787	2937.740679	22.894323
106.228969	2940.493694	22.899341
106.029814	2954.922119	22.904359
106.322674	2955.005439	22.909376
106.361330	2963.638790	22.914394
106.387408	2971.703863	22.919411
106.864584	2962.404265	22.924429
106.677114	2966.486194	22.929447
106.917153	2960.731885	22.934464
106.755163	2971.597371	22.939482
106.702689	2990.726010	22.944499
107.000776	2996.387901	22.949517
107.193761	2994.456915	22.954535
107.390383	2987.017528	22.959552
107.385222	2995.796328	22.964570
107.901580	3008.101715	22.969587
108.308878	3001.639518	22.974605
107.974039	3010.643164	22.979623
108.149192	3006.290694	22.984640
108.577477	3012.194557	22.989658
108.243537	3010.020363	22.994675
108.381143	3007.354862	22.999693
108.482776	3015.030339	23.004711
108.870807	3000.960782	23.009728
108.778392	3005.772481	23.014746
108.424299	3001.011203	23.019763
108.794683	3003.865180	23.024781
108.741775	3017.516776	23.029799
109.054376	3030.634988	23.034816
109.133189	3029.950887	23.039834
109.070631	3038.594915	23.044851
109.599146	3028.811191	23.049869
109.314060	3027.444131	23.054887
109.805034	3026.698240	23.059904
109.824440	3028.923839	23.064922
109.665938	3033.272547	23.069939
110.253320	3031.214951	23.074957
110.097689	3054.520499	23.079975
110.345971	3053.461691	23.084992
110.545141	3056.888888	23.090010
110.384586	3049.625202	23.095027
110.625048	3059.187668	23.100045
110.368986	3066.593766	23.105063
110.604234	3050.934398	23.110080
110.843430	3055.055295	23.115098
110.503253	3056.188999	23.120115
110.698319	3062.154456	23.125133
110.939543	3076.697632	23.130151
110.937338	3078.544391	23.135168
110.828048	3084.386909	23.140186
110.802103	3082.947057	23.145203
111.117067	3098.627736	23.150221
111.285438	3104.557350	23.155239
111.547094	3106.546892	23.160256
111.727200	3106.965199	23.165274
111.697352	3115.119503	23.170291
112.023878	3115.737861	23.175309
111.941954	3126.733858	23.180327
112.060996	3133.798569	23.185344
112.611863	3142.919073	23.190362
112.526050	3141.404593	23.195379
112.721566	3135.651024	23.200397
112.583550	3143.305786	23.205415
112.546563	3138.965866	23.210432
113.007215	3149.829739	23.215450
113.469078	3166.221766	23.220467
113.779310	3155.959104	23.225485
113.682012	3160.803884	23.230503
113.436122	3156.468166	23.235520
113.861889	3155.171810	23.240538
113.968187	3152.105381	23.245555
113.949328	3143.608453	23.250573
113.657866	3148.208875	23.255591
114.092628	3148.006054	23.260608
114.140855	3145.822816	23.265626
113.823104	3152.221701	23.270643
114.277523	3141.866048	23.275661
114.109814	3144.208816	23.280679
114.255751	3157.145266	23.285696
114.351311	3165.441644	23.290714
114.381264	3176.224758	23.295731
114.609870	3173.093198	23.300749
114.683043	3182.185278	23.305767
114.790197	3193.771817	23.310784
114.947876	3197.506938	23.315802
114.639007	3203.940613	23.320819
115.401793	3203.599745	23.325837
115.294564	3228.395572	23.330855
115.608885	3229.118929	23.335872
115.862753	3224.518645	23.340890
115.876082	3227.365886	23.345907
116.168796	3220.342913	23.350925
115.897755	3227.119038	23.355943
116.177055	3228.152401	23.360960
116.729111	3246.537590	23.365978
116.596115	3249.032163	23.370995
116.826503	3239.525532	23.376013
117.353349	3247.038934	23.381031
117.067297	3245.883607	23.386048
116.900479	3240.736048	23.391066
117.185534	3245.320872	23.396083
116.977926	3229.592698	23.401101
116.900007	3239.423157	23.406119
116.852986	3238.016542	23.411136
117.158260	3230.369345	23.416154
117.234241	3246.251908	23.421171
117.521870	3253.071901	23.426189
117.324000	3267.981053	23.431207
117.786242	3267.873752	23.436224
117.626373	3264.464297	23.441242
117.827787	3285.364427	23.446259
117.938679	3296.198439	23.451277
118.191369	3301.977031	23.456295
118.047132	3295.737951	23.461312
118.327617	3302.345144	23.466330
118.488078	3332.541900	23.471347
118.725352	3324.875606	23.476365
119.033722	3321.131888	23.481383
118.839081	3327.464020	23.486400
118.801810	3332.141173	23.491418
118.703670	3341.937167	23.496435
119.275278	3347.890685	23.501453
119.429104	3366.059487	23.506471
119.443470	3353.840326	23.511488
119.747035	3353.699330	23.516506
120.131778	3364.290709	23.521523
120.095490	3380.972441	23.526541
120.221120	3389.108399	23.531559
120.054073	3387.982068	23.536576
120.265040	3379.691424	23.541594
120.300618	3381.955403	23.546611
120.626096	3369.471871	23.551629
120.626376	3379.822502	23.556647
121.043046	3394.798984	23.561664
121.197016	3396.802592	23.566682
121.157749	3410.637236	23.571699
121.400064	3394.112657	23.576717
121.445252	3397.765078	23.581735
121.166246	3399.415306	23.586752
121.422470	3390.034252	23.591770
121.710108	3393.175249	23.596787
122.137446	3385.859345	23.601805
121.863665	3394.313075	23.606823
122.096803	3418.686023	23.611840
122.155158	3406.069636	23.616858
121.893274	3413.675066	23.621875
122.300633	3418.226285	23.626893
122.617463	3407.812150	23.631911
122.579787	3410.646321	23.636928
122.859869	3425.239500	23.641946
122.838757	3444.691756	23.646963
123.062893	3437.311472	23.651981
123.330101	3441.966069	23.656999
123.237462	3440.967890	23.662016
123.490016	3440.835814	23.667034
123.439521	3444.689149	23.672051
123.507284	3433.768001	23.677069
123.655520	3435.876364	23.682087
123.521993	3445.299700	23.687104
123.585629	3461.488892	23.692122
123.839455	3463.110016	23.697139
123.963748	3452.420551	23.702157
124.241248	3462.342373	23.707175
124.020062	3468.395610	23.712192
124.660599	3480.368520	23.717210
124.406185	3498.731590	23.722227
124.745760	3491.896102	23.727245
124.629818	3490.624740	23.732263
124.362065	3492.391965	23.737280
124.719128	3505.682084	23.742298
124.813383	3518.420996	23.747315
125.129093	3518.300089	23.752333
125.222870	3524.403029	23.757351
125.375811	3551.285768	23.762368
125.768929	3551.667764	23.767386
125.844924	3551.585866	23.772403
125.858626	3552.642725	23.777421
126.410777	3557.452517	23.782439
126.339199	3547.851455	23.787456
126.645977	3540.412317	23.792474
126.670476	3557.010613	23.797491
126.804515	3557.323791	23.802509
127.267442	3561.136196	23.807527
127.299810	3562.131081	23.812544
127.358367	3557.799401	23.817562
127.473127	3562.785920	23.822579
126.908885	3561.032241	23.827597
127.265759	3568.484811	23.832615
127.341424	3562.770639	23.837632
127.518367	3559.426191	23.842650
127.412584	3572.204127	23.847667
127.715427	3580.545567	23.852685
127.531125	3592.051460	23.857703
127.643535	3603.053799	23.862720
128.260173	3600.959213	23.867738
128.401486	3616.019948	23.872755
128.269535	3619.367135	23.877773
128.696002	3614.629079	23.882791
128.463058	3628.671019	23.887808
128.690646	3620.982516	23.892826
128.903119	3634.970746	23.897843
129.127032	3646.348659	23.902861
129.390930	3649.902552	23.907879
128.868730	3655.599528	23.912896
129.562150	3657.419613	23.917914
129.768727	3655.802606	23.922931
129.443959	3676.458379	23.927949
129.445016	3680.723624	23.932967
129.467714	3674.285488	23.937984
129.757363	3670.724810	23.943002
130.081251	3695.040484	23.948019
130.337948	3699.692120	23.953037
130.386216	3691.321833	23.958055
130.523580	3700.099569	23.963072
130.781904	3703.513555	23.968090
130.885721	3725.085938	23.973107
130.821110	3728.236763	23.978125
131.181156	3728.446257	23.983143
131.190798	3731.974633	23.988160
131.485664	3718.060845	23.993178
131.137476	3723.888216	23.998195
131.537783	3736.715396	24.003213
132.322212	3749.129707	24.008231
132.197974	3750.601112	24.013248
132.373597	3746.811590	24.018266
132.368660	3744.208018	24.023283
132.374252	3748.965787	24.028301
132.775360	3753.223117	24.033319
132.660223	3742.131095	24.038336
132.971673	3739.905012	24.043354
132.581033	3742.563465	24.048371
132.807372	3736.778002	24.053389
133.095327	3735.795421	24.058407
132.817877	3744.866667	24.063424
133.028232	3764.528661	24.068442
133.240165	3769.528076	24.073459
133.079778	3774.236801	24.078477
133.472001	3789.505501	24.083495
133.580700	3796.320455	24.088512
133.945077	3798.567470	24.093530
133.933132	3809.036778	24.098547
134.106971	3821.450965	24.103565
134.683634	3824.756008	24.108583
134.481754	3834.661697	24.113600
134.765104	3829.617573	24.118618
134.710501	3817.603326	24.123635
134.698430	3829.491000	24.128653
134.974428	3841.722932	24.133671
135.295663	3849.219089	24.138688
135.583746	3855.412331	24.143706
135.409208	3850.880949	24.148723
135.727100	3848.720688	24.153741
135.917015	3847.823745	24.158759
135.693495	3854.930053	24.163776
135.799585	3865.701535	24.168794
136.049846	3878.894959	24.173811
136.216853	3877.125334	24.178829
136.355707	3872.610841	24.183847
136.453010	3884.428415	24.188864
136.863262	3887.118883	24.193882
137.001764	3902.772713	24.198899
136.971328	3910.582211	24.203917
137.091131	3899.352704	24.208935
137.139327	3900.909121	24.213952
137.044263	3898.662874	24.218970
137.297237	3910.203131	24.223987
137.632652	3918.309868	24.229005
138.134078	3919.065576	24.234023
137.702638	3933.211828	24.239040
137.893989	3920.327569	24.244058
137.857199	3924.266950	24.249075
137.891017	3934.111524	24.254093
138.343546	3942.695195	24.259111
138.303434	3952.894553	24.264128
138.168570	3956.960499	24.269146
138.527878	3952.182700	24.274163
138.860021	3972.613786	24.279181
139.347334	3972.673982	24.284199
139.499228	3966.813766	24.289216
139.669971	3965.524184	24.294234
139.804369	3961.633408	24.299251
139.835426	3970.753148	24.304269
140.024557	3955.102531	24.309287
139.935390	3958.641210	24.314304
139.990002	3959.067755	24.319322
139.994776	3963.838311	24.324339
140.028038	3984.343030	24.329357
140.325162	3986.670025	24.334375
140.101172	3994.477390	24.339392
140.517745	3998.652088	24.344410
140.934278	4011.480070	24.349427
140.849068	4026.202108	24.354445
141.088945	4022.013660	24.359463
141.191079	4017.926628	24.364480
141.170762	4021.446478	24.369498
141.578514	4037.764731	24.374515
141.331936	4052.797297	24.379533
141.746554	4053.806001	24.384551
141.734927	4057.657232	24.389568
141.981261	4068.229502	24.394586
142.248963	4070.967122	24.399603
142.343148	4072.789984	24.404621
142.226924	4080.510198	24.409639
142.262572	4097.401540	24.414656
142.524163	4108.172006	24.419674
142.908263	4107.569767	24.424691
143.136053	4105.747943	24.429709
143.585794	4095.269653	24.434727
143.613794	4115.158647	24.439744
143.686520	4123.727464	24.444762
144.020275	4119.649887	24.449779
143.860663	4123.163651	24.454797
144.309281	4116.843851	24.459815
144.385492	4109.088765	24.464832
144.655929	4116.280853	24.469850
144.812840	4111.417275	24.474867
144.930428	4108.460555	24.479885
145.072491	4111.370042	24.484903
144.648800	4124.784426	24.489920
144.840314	4110.440707	24.494938
145.251042	4119.813883	24.499955
145.022301	4142.169933	24.504973
145.100183	4133.111057	24.509991
145.580377	4140.310620	24.515008
145.547800	4139.091201	24.520026
145.743362	4132.113968	24.525043
145.557285	4146.272435	24.530061
146.005085	4152.244458	24.535079
145.856851	4163.057496	24.540096
145.993089	4166.203923	24.545114
146.447216	4177.317411	24.550131
146.164157	4196.072171	24.555149
146.465016	4191.535684	24.560167
146.832820	4200.915756	24.565184
146.732203	4203.390379	24.570202
147.050073	4216.028165	24.575219
147.272847	4224.271820	24.580237
147.642016	4224.224989	24.585255
147.629744	4225.371785	24.590272
147.731312	4234.419872	24.595290
148.218237	4237.571761	24.600307
148.105402	4249.967513	24.605325
148.328245	4253.200059	24.610343
148.428304	4243.675802	24.615360
148.900452	4240.995287	24.620378
148.684319	4247.920457	24.625395
148.481405	4244.634061	24.630413
148.824992	4247.765540	24.635431
149.059024	4261.044498	24.640448
149.100364	4271.769176	24.645466
149.257959	4264.650039	24.650483
149.358544	4281.326704	24.655501
149.703851	4289.218096	24.660519
149.952531	4295.030764	24.665536
149.734909	4299.301161	24.670554
149.852542	4307.327985	24.675571
150.098173	4318.987737	24.680589
150.635505	4320.634560	24.685607
150.557193	4322.442476	24.690624
150.472194	4320.883689	24.695642
151.274240	4330.093913	24.700659
151.084302	4348.863914	24.705677
151.152371	4344.860892	24.710695
151.402439	4338.757526	24.715712
150.984184	4346.359259	24.720730
151.536040	4351.775899	24.725747
151.676266	4357.479229	24.730765
151.886192	4363.113234	24.735783
151.844965	4365.180353	24.740800
151.847405	4375.940416	24.745818
152.322529	4393.314279	24.750835
152.485579	4402.480109	24.755853
152.638287	4389.272769	24.760871
153.004621	4402.133487	24.765888
153.271741	4416.832781	24.770906
153.119420	4421.554584	24.775923
153.471250	4419.578424	24.780941
153.414442	4418.252709	24.785959
153.805108	4423.703730	24.790976
153.642369	4427.028473	24.795994
153.875915	4414.059175	24.801011
153.798238	4423.491538	24.806029
153.819421	4434.080305	24.811047
154.321204	4446.661434	24.816064
154.156324	4439.729725	24.821082
154.428352	4448.222900	24.826099
154.630822	4467.614116	24.831117
154.518422	4462.162440	24.836135
155.150478	4467.578924	24.841152
154.864094	4475.389409	24.846170
155.248207	4492.003013	24.851187
155.364169	4492.750988	24.856205
155.554034	4491.972806	24.861223
155.735659	4499.998186	24.866240
155.826112	4511.172274	24.871258
156.303585	4513.964642	24.876275
155.902108	4520.666177	24.881293
156.436137	4518.763223	24.886311
156.522816	4533.201115	24.891328
156.779520	4544.057645	24.896346
157.050988	4543.590567	24.901363
157.165300	4551.750218	24.906381
157.216683	4553.397453	24.911399
157.492435	4551.350016	24.916416
157.819838	4565.539512	24.921434
157.925791	4570.411350	24.926451
157.849525	4575.248521	24.931469
158.114520	4571.091315	24.936487
158.182343	4566.239432	24.941504
158.297496	4575.581360	24.946522
158.475433	4578.155597	24.951539
158.687643	4595.071282	24.956557
158.853606	4598.608771	24.961575
159.030588	4591.586296	24.966592
158.779577	4609.605635	24.971610
158.939951	4614.246176	24.976627
159.236372	4627.522600	24.981645
159.496948	4631.292034	24.986663
159.652832	4629.239311	24.991680
159.473183	4648.355772	24.996698
159.786169	4652.488962	25.001715
159.914446	4662.811436	25.006733
160.047056	4673.930937	25.011751
160.477608	4686.476428	25.016768
160.448384	4681.398464	25.021786
160.746996	4688.904956	25.026803
160.880560	4704.716982	25.031821
161.066899	4714.203415	25.036839
161.343532	4715.740805	25.041856
161.517751	4717.818466	25.046874
161.815702	4718.966974	25.051891
162.064590	4731.864803	25.056909
162.542331	4728.148801	25.061927
162.904297	4720.670381	25.066944
162.513853	4725.352363	25.071962
163.034094	4718.607875	25.076979
162.848422	4722.299795	25.081997
163.059623	4714.983087	25.087015
163.452376	4714.860909	25.092032
162.991024	4727.567519	25.097050
163.436249	4716.669415	25.102067
163.273918	4715.675178	25.107085
163.420022	4711.264691	25.112103
163.489179	4715.441496	25.117120
163.654751	4733.079099	25.122138
163.996281	4734.479486	25.127155
163.718702	4748.557141	25.132173
163.989033	4757.197094	25.137191
164.403950	4763.998291	25.142208
164.169628	4776.351705	25.147226
164.454209	4767.085624	25.152243
164.605217	4789.609465	25.157261
164.693258	4803.220580	25.162279
164.874031	4803.965318	25.167296
165.277599	4832.874759	25.172314
165.478519	4826.414785	25.177331
165.707401	4836.497130	25.182349
165.700639	4851.384494	25.187367
166.278977	4857.272274	25.192384
166.189648	4859.803422	25.197402
166.670302	4852.922791	25.202419
166.690002	4858.399294	25.207437
166.772330	4870.848629	25.212455
166.832832	4878.323952	25.217472
167.307745	4888.736860	25.222490
167.310874	4876.364816	25.227507
167.382011	4891.043123	25.232525
167.350219	4911.944995	25.237543
167.678017	4907.164050	25.242560
167.576831	4908.022192	25.247578
167.776746	4928.862757	25.252595
167.800083	4942.328548	25.257613
168.245452	4938.599563	25.262631
168.849359	4952.402344	25.267648
168.700479	4976.429701	25.272666
168.814328	4974.260906	25.277683
168.955670	4980.756521	25.282701
169.099610	4991.907499	25.287719
169.609140	4995.294329	25.292736
169.701325	4998.949097	25.297754
169.692377	4985.237540	25.302771
170.398015	4993.421167	25.307789
170.392749	4996.222152	25.312807
170.617120	5002.106637	25.317824
170.433209	5019.069445	25.322842
171.013252	5015.042046	25.327859
171.030098	5011.341242	25.332877
170.941034	5011.011877	25.337895
171.077138	5004.581827	25.342912
171.250282	5014.444248	25.347930
171.189114	5022.168763	25.352947
171.551341	5033.969413	25.357965
171.412420	5036.766541	25.362983
171.815060	5026.609794	25.368000
171.932386	5065.816243	25.373018
172.363734	5067.397450	25.378035
172.660162	5064.754250	25.383053
172.386848	5069.888909	25.388071
172.418378	5074.624090	25.393088
172.793647	5088.761620	25.398106
172.881166	5097.035987	25.403123
173.138387	5107.158056	25.408141
173.216443	5118.724796	25.413159
173.530210	5121.724332	25.418176
173.481415	5132.791283	25.423194
173.579432	5130.070351	25.428211
174.010749	5145.206789	25.433229
174.249271	5156.663009	25.438247
174.667757	5138.467287	25.443264
174.974233	5168.476184	25.448282
174.930182	5171.128403	25.453299
175.255444	5181.264064	25.458317
175.266961	5185.639792	25.463335
175.378300	5178.691231	25.468352
175.321937	5181.586151	25.473370
175.588331	5193.773543	25.478387
176.299849	5185.732510	25.483405
176.095717	5191.588621	25.488423
176.468573	5188.532772	25.493440
176.413510	5191.912896	25.498458
176.530950	5210.088998	25.503475
176.839559	5217.233849	25.508493
176.736297	5228.589630	25.513511
177.290768	5220.390310	25.518528
177.481828	5231.351437	25.523546
177.600744	5242.383078	25.528563
177.834822	5237.261370	25.533581
177.526799	5244.644582	25.538599
177.916512	5245.512592	25.543616
178.009265	5265.499812	25.548634
178.337308	5276.344725	25.553651
178.388770	5280.339630	25.558669
178.198663	5284.580746	25.563687
178.714566	5298.004521	25.568704
179.026188	5309.184864	25.573722
179.166816	5318.007107	25.578739
179.632160	5327.030914	25.583757
179.610929	5339.291818	25.588775
179.839227	5329.432510	25.593792
179.940811	5327.449714	25.598810
180.139522	5340.325395	25.603827
180.177689	5353.420220	25.608845
180.469081	5353.523472	25.613863
180.749339	5349.631895	25.618880
180.423591	5350.719400	25.623898
180.882366	5366.022411	25.628915
181.090300	5378.427761	25.633933
180.829853	5391.043114	25.638951
180.877656	5396.902410	25.643968
181.414804	5411.294521	25.648986
181.499542	5418.881905	25.654003
181.857689	5425.860826	25.659021
182.051321	5437.844455	25.664039
182.388672	5439.511497	25.669056
182.516171	5444.909666	25.674074
182.738937	5452.032127	25.679092
183.230709	5459.084169	25.684109
183.340745	5465.167232	25.689127
183.324687	5468.361824	25.694144
183.610731	5461.850240	25.699162
183.667042	5474.458434	25.704180
183.759496	5497.361675	25.709197
183.724643	5505.711639	25.714215
184.208272	5491.966711	25.719232
184.435761	5506.665549	25.724250
184.522786	5519.382962	25.729268
185.116478	5518.091907	25.734285
185.077810	5527.312629	25.739303
185.065541	5519.855709	25.744320
185.392645	5534.605567	25.749338
185.609698	5546.709070	25.754356
185.685387	5548.371424	25.759373
185.977883	5552.958157	25.764391
186.373076	5546.787103	25.769408
186.195110	5568.212790	25.774426
186.090259	5572.145365	25.779444
186.427411	5577.813056	25.784461
186.646222	5595.847593	25.789479
186.715155	5611.428580	25.794496
186.866145	5610.700600	25.799514
187.007930	5616.555227	25.804532
187.645283	5625.233950	25.809549
187.658995	5634.876740	25.814567
188.113093	5631.526981	25.819584
188.078177	5652.246299	25.824602
187.975975	5665.667464	25.829620
188.575085	5659.872964	25.834637
188.340318	5670.382265	25.839655
188.486708	5680.309191	25.844672
189.183413	5688.678737	25.849690
189.115639	5690.442654	25.854708
189.031283	5703.827178	25.859725
189.311397	5727.187070	25.864743
189.679769	5722.389171	25.869760
189.590555	5736.997113	25.874778
189.587120	5746.843331	25.879796
190.324468	5766.064444	25.884813
190.518136	5778.013727	25.889831
190.733408	5768.278939	25.894848
190.940914	5770.308960	25.899866
191.313896	5770.809111	25.904884
191.422121	5769.825165	25.909901
191.448471	5793.464791	25.914919
191.864889	5787.076257	25.919936
191.804110	5791.742203	25.924954
191.816472	5785.019201	25.929972
192.167323	5790.820112	25.934989
192.295442	5810.025116	25.940007
192.490035	5814.439505	25.945024
192.735394	5816.816753	25.950042
192.950798	5816.705540	25.955060
193.279541	5838.823433	25.960077
192.956510	5851.705637	25.965095
193.026639	5854.434185	25.970112
193.497849	5862.011323	25.975130
193.433730	5881.557051	25.980148
193.743061	5885.214400	25.985165
193.886953	5912.439634	25.990183
194.138493	5916.503519	25.995200
194.367339	5921.808603	26.000218
194.870608	5932.376663	26.005236
195.133522	5942.533807	26.010253
195.369064	5948.745760	26.015271
195.786748	5950.277321	26.020288
196.209891	5958.272864	26.025306
196.049949	5959.735227	26.030324
196.715031	5949.790139	26.035341
196.378851	5961.714681	26.040359
196.639931	5955.014105	26.045376
196.701416	5954.881798	26.050394
196.835924	5975.462838	26.055412
197.244941	5980.313579	26.060429
196.980599	5984.052182	26.065447
197.116637	5997.403409	26.070464
197.578324	5999.790258	26.075482
197.526308	6015.727691	26.080500
197.725282	6027.018591	26.085517
198.006578	6048.616441	26.090535
197.986150	6053.519934	26.095552
198.632563	6054.690107	26.100570
198.585456	6069.327069	26.105588
198.752287	6060.576196	26.110605
198.884837	6080.443306	26.115623
198.728493	6088.724849	26.120640
199.323500	6097.815794	26.125658
199.243863	6123.682890	26.130676
199.702919	6117.792528	26.135693
200.051826	6140.075241	26.140711
200.189458	6155.927515	26.145728
200.473114	6156.772369	26.150746
200.447729	6164.274624	26.155764
201.152731	6171.219849	26.160781
201.099479	6182.888607	26.165799
201.286286	6175.795369	26.170816
201.641574	6190.871838	26.175834
201.672033	6203.380921	26.180852
202.038265	6198.194544	26.185869
202.079010	6204.938838	26.190887
202.492880	6201.233451	26.195904
202.724950	6217.636430	26.200922
202.536829	6237.228359	26.205940
202.899255	6234.129905	26.210957
202.990505	6235.555396	26.215975
203.149178	6252.678217	26.220992
203.526259	6265.435791	26.226010
203.515221	6268.387427	26.231028
203.694294	6277.927956	26.236045
204.033392	6289.308442	26.241063
204.141759	6288.125384	26.246080
204.410484	6303.011991	26.251098
204.430175	6314.648767	26.256116
204.726822	6310.556060	26.261133
204.824188	6322.359060	26.266151
205.139806	6347.221753	26.271168
205.752232	6341.013383	26.276186
205.829948	6346.987879	26.281204
206.105150	6355.749164	26.286221
206.045956	6372.735337	26.291239
206.379735	6381.136392	26.296256
206.602323	6378.769097	26.301274
206.866597	6393.041237	26.306292
207.119369	6395.276563	26.311309
207.158204	6401.233676	26.316327
207.230965	6409.806178	26.321344
207.654229	6420.130852	26.326362
207.874897	6424.358733	26.331380
208.530862	6429.545557	26.336397
208.905150	6430.597067	26.341415
209.128004	6422.922035	26.346432
208.934582	6428.435455	26.351450
208.854258	6446.743743	26.356468
209.241552	6447.734171	26.361485
209.119060	6453.814586	26.366503
208.986965	6468.307345	26.371520
209.396506	6478.561076	26.376538
209.565068	6489.306424	26.381556
209.764550	6507.224777	26.386573
210.084000	6510.340931	26.391591
210.212491	6509.367869	26.396608
210.486974	6529.053235	26.401626
210.873431	6537.459357	26.406644
210.921169	6540.978399	26.411661
211.485082	6561.660961	26.416679
211.820641	6561.247344	26.421696
212.279583	6558.052399	26.426714
212.277028	6565.337995	26.431732
212.640978	6571.020684	26.436749
212.475138	6592.438047	26.441767
212.452714	6590.540945	26.446784
212.575503	6576.109808	26.451802
212.891773	6590.193672	26.456820
213.397685	6598.096118	26.461837
213.523383	6611.181249	26.466855
213.529098	6620.668595	26.471872
213.695747	6613.450902	26.476890
214.103531	6637.437845	26.481908
214.150357	6637.430610	26.486925
214.367998	6638.895789	26.491943
214.232815	6647.009040	26.496960
214.639483	6661.640339	26.501978
214.441072	6675.928288	26.506996
214.885377	6682.646232	26.512013
215.244220	6708.354751	26.517031
215.242120	6726.001798	26.522048
216.004911	6731.452591	26.527066
215.959130	6748.982313	26.532084
216.384491	6752.488415	26.537101
216.197565	6767.787242	26.542119
216.614036	6776.169833	26.547136
216.894268	6795.761795	26.552154
216.843346	6797.753691	26.557172
217.179695	6799.847507	26.562189
217.598520	6819.400884	26.567207
217.610705	6833.820642	26.572224
218.308589	6834.502726	26.577242
218.271603	6850.983133	26.582260
218.323818	6852.636001	26.587277
218.467841	6857.607962	26.592295
219.150937	6877.018574	26.597312
219.481790	6872.716478	26.602330
219.483479	6880.937862	26.607348
219.633883	6895.887990	26.612365
219.841977	6900.781299	26.617383
219.798428	6910.017034	26.622400
220.286274	6912.182708	26.627418
220.662137	6930.544760	26.632436
221.165118	6933.110088	26.637453
220.974737	6940.127606	26.642471
221.369698	6939.379556	26.647488
221.621243	6952.111316	26.652506
221.507170	6950.330277	26.657524
221.460281	6947.435410	26.662541
222.181023	6963.856522	26.667559
222.247999	6986.118576	26.672576
222.276654	6989.089992	26.677594
222.477018	6997.107455	26.682612
222.879439	7007.163625	26.687629
223.428875	7010.571329	26.692647
223.603384	7023.386245	26.697664
223.636558	7031.789169	26.702682
223.876582	7036.199045	26.707700
223.999063	7038.212114	26.712717
224.193188	7045.863939	26.717735
224.509034	7063.090895	26.722752
225.023930	7053.765437	26.727770
224.919753	7060.314486	26.732788
224.999870	7071.263981	26.737805
225.346655	7082.133993	26.742823
225.309024	7090.995942	26.747840
225.394410	7089.051691	26.752858
225.532032	7118.468303	26.757876
226.099061	7121.021882	26.762893
226.397678	7139.800936	26.767911
226.002708	7151.052830	26.772928
226.403535	7161.086542	26.777946
226.562626	7173.937880	26.782964
226.514597	7192.413465	26.787981
227.378151	7203.690598	26.792999
227.422082	7224.037599	26.798016
227.795172	7226.987990	26.803034
228.115357	7241.336227	26.808052
228.151489	7263.679149	26.813069
228.828790	7261.251822	26.818087
228.690521	7285.069566	26.823104
229.147330	7279.056366	26.828122
229.273529	7304.912377	26.833140
229.511782	7300.971130	26.838157
229.723002	7314.660129	26.843175
229.924435	7332.125950	26.848192
230.290620	7333.269310	26.853210
230.763856	7339.211843	26.858228
230.599244	7367.330845	26.863245
230.772609	7345.057121	26.868263
230.967710	7374.576022	26.873280
231.174252	7381.849144	26.878298
231.545567	7402.239803	26.883316
231.971306	7405.250293	26.888333
232.361218	7409.745759	26.893351
232.158395	7420.855493	26.898368
232.524809	7430.258318	26.903386
233.015425	7440.577695	26.908404
233.017109	7445.123256	26.913421
233.280941	7457.693763	26.918439
233.410479	7468.674228	26.923456
233.704591	7463.608287	26.928474
233.875645	7489.047521	26.933492
234.168376	7487.304647	26.938509
234.434708	7519.419303	26.943527
234.798374	7528.083778	26.948544
234.864275	7532.339010	26.953562
235.155600	7527.817205	26.958580
235.398703	7544.786428	26.963597
235.873210	7557.426514	26.968615
236.005907	7568.537953	26.973632
236.172482	7572.525357	26.978650
236.274153	7595.034584	26.983668
236.373264	7587.040335	26.988685
236.574525	7602.326922	26.993703
236.562107	7617.189639	26.998720
237.164288	7614.445329	27.003738
237.397136	7630.995319	27.008756
237.384730	7653.206502	27.013773
237.617666	7652.430744	27.018791
237.809496	7674.643238	27.023808
238.207774	7678.769204	27.028826
238.243807	7691.443105	27.033844
238.757418	7711.161954	27.038861
238.865621	7701.675098	27.043879
239.093165	7718.897221	27.048896
239.270224	7735.250063	27.053914
239.408665	7745.030139	27.058932
239.685842	7757.048758	27.063949
240.286676	7767.420038	27.068967
240.348242	7786.843582	27.073984
240.691432	7804.453391	27.079002
241.015508	7803.131964	27.084020
241.151538	7811.658209	27.089037
241.612886	7809.883699	27.094055
241.646488	7829.927084	27.099072
241.929719	7841.375116	27.104090
242.371542	7849.540252	27.109108
242.303507	7860.253491	27.114125
242.753758	7867.931798	27.119143
242.728424	7872.890966	27.124160
242.980745	7877.142548	27.129178
243.502506	7893.138460	27.134196
243.646990	7909.734321	27.139213
244.060637	7911.478413	27.144231
244.074016	7919.182320	27.149248
244.648261	7923.206341	27.154266
244.508308	7928.676379	27.159284
244.590029	7955.635146	27.164301
245.190529	7950.583153	27.169319
245.154065	7971.176904	27.174336
245.269851	7989.505399	27.179354
245.861883	8003.427835	27.184372
245.847145	8023.032241	27.189389
246.309917	8020.353361	27.194407
246.321948	8049.749342	27.199424
246.607996	8050.806389	27.204442
247.228367	8056.185178	27.209460
247.397932	8081.454123	27.214477
247.641085	8078.733914	27.219495
247.435401	8089.230835	27.224512
248.054142	8109.367027	27.229530
248.450490	8104.185429	27.234548
248.534293	8125.537658	27.239565
248.716962	8129.726449	27.244583
248.768487	8152.091069	27.249600
249.184196	8169.157032	27.254618
249.727818	8168.033497	27.259636
249.565185	8182.069313	27.264653
250.031524	8191.199384	27.269671
250.030503	8205.986116	27.274688
250.241077	8209.652712	27.279706
250.559217	8224.729309	27.284724
250.398955	8231.487679	27.289741
251.211891	8247.242412	27.294759
251.135957	8268.689161	27.299776
251.389471	8280.983846	27.304794
251.884949	8286.500661	27.309812
252.054110	8295.198558	27.314829
252.276749	8306.379229	27.319847
252.530005	8323.981563	27.324864
252.584266	8328.694095	27.329882
253.066102	8332.782535	27.334900
253.076628	8357.092110	27.339917
253.661417	8364.849953	27.344935
253.813707	8385.603435	27.349952
253.812355	8395.979474	27.354970
254.324334	8403.528613	27.359988
254.346521	8423.679272	27.365005
254.729577	8437.437916	27.370023
255.474841	8436.637113	27.375040
255.637254	8459.250488	27.380058
255.952943	8454.726884	27.385076
256.035239	8475.916180	27.390093
256.466932	8474.941092	27.395111
256.831421	8481.222873	27.400128
256.704678	8492.449538	27.405146
257.285250	8495.568171	27.410164
257.518388	8499.453148	27.415181
257.848720	8508.368238	27.420199
257.969765	8518.746493	27.425216
258.093587	8529.829376	27.430234
258.284288	8550.116627	27.435252
258.306984	8555.989435	27.440269
258.616860	8570.107679	27.445287
258.780750	8576.979784	27.450304
258.781258	8601.731626	27.455322
259.510243	8601.069153	27.460340
259.685081	8626.970459	27.465357
259.911819	8635.646787	27.470375
260.453059	8654.165602	27.475392
260.543665	8667.682280	27.480410
260.649844	8671.111459	27.485428
261.036117	8697.218799	27.490445
261.149485	8697.126989	27.495463
261.613989	8720.154917	27.500480
261.765757	8736.801293	27.505498
262.108409	8751.629001	27.510516
262.423741	8757.496557	27.515533
262.616666	8773.196444	27.520551
262.750015	8789.502720	27.525568
263.203713	8784.697339	27.530586
263.465267	8802.041593	27.535604
263.604426	8821.829475	27.540621
264.017696	8827.925392	27.545639
264.270732	8838.527955	27.550656
264.442687	8847.929628	27.555674
264.999695	8845.042793	27.560692
264.950143	8874.408110	27.565709
264.949235	8874.284938	27.570727
265.583807	8891.445114	27.575744
265.704309	8896.516333	27.580762
265.938525	8906.159539	27.585780
265.694861	8928.714805	27.590797
266.073669	8930.537367	27.595815
266.594782	8950.114235	27.600832
266.851251	8975.174109	27.605850
267.253054	8977.780331	27.610868
267.352738	8989.831386	27.615885
267.767186	9007.671667	27.620903
268.293945	9029.759216	27.625920
267.845094	9036.480138	27.630938
268.686627	9039.779601	27.635956
268.453807	9064.321516	27.640973
269.000655	9068.257367	27.645991
269.396418	9091.080026	27.651008
269.694822	9111.568065	27.656026
269.777916	9120.507586	27.661044
269.981479	9129.932334	27.666061
270.273202	9147.034134	27.671079
270.282218	9161.354738	27.676096
270.727191	9177.177378	27.681114
271.195576	9195.606964	27.686132
271.511173	9215.846488	27.691149
271.964133	9222.030675	27.696167
272.307215	9235.020902	27.701184
272.601564	9257.978021	27.706202
273.148847	9271.109646	27.711220
273.076606	9266.062151	27.716237
273.139663	9288.169694	27.721255
273.546333	9294.486020	27.726272
273.739983	9312.797826	27.731290
274.363834	9311.873510	27.736308
274.446209	9319.451461	27.741325
274.674213	9343.445459	27.746343
275.195724	9345.276414	27.751360
275.008758	9365.426264	27.756378
275.343930	9379.359065	27.761396
275.665256	9404.444340	27.766413
275.865767	9418.507633	27.771431
276.485134	9430.534444	27.776448
276.206579	9451.880219	27.781466
276.615648	9448.433724	27.786484
277.210299	9475.805711	27.791501
277.350743	9481.386256	27.796519
278.059056	9496.233544	27.801536
278.000085	9505.470191	27.806554
278.411529	9519.317779	27.811572
278.596868	9525.666334	27.816589
278.694348	9539.842958	27.821607
279.214737	9547.083251	27.826624
279.302992	9562.953714	27.831642
279.746281	9554.352691	27.836660
279.872579	9566.630546	27.841677
280.347907	9577.049076	27.846695
280.802732	9590.281105	27.851712
280.720698	9600.066061	27.856730
281.367675	9594.862505	27.861748
281.725279	9614.141687	27.866765
281.624457	9620.454050	27.871783
281.878705	9634.185147	27.876800
282.193586	9635.895617	27.881818
282.477631	9640.105665	27.886836
282.512770	9655.384242	27.891853
282.878557	9679.466600	27.896871
283.178976	9680.981853	27.901888
283.010617	9701.175618	27.906906
283.493455	9714.974234	27.911924
283.759920	9729.855194	27.916941
284.267289	9753.167881	27.921959
284.294586	9763.133045	27.926976
284.435652	9781.296018	27.931994
284.744304	9787.539644	27.937012
285.373638	9811.555025	27.942029
285.591353	9836.427743	27.947047
286.001830	9835.807341	27.952064
286.198117	9862.437674	27.957082
286.718887	9867.918790	27.962100
287.082996	9868.764036	27.967117
287.284768	9890.772054	27.972135
287.488166	9893.118885	27.977152
287.303344	9922.280769	27.982170
288.035300	9925.956374	27.987188
288.212995	9948.822576	27.992205
288.109894	9954.895020	27.997223
288.620164	9970.153276	28.002240
288.818521	9997.339911	28.007258
289.056186	10011.650853	28.012276
289.359891	10041.377279	28.017293
290.065937	10058.530557	28.022311
290.647657	10074.877733	28.027328
290.443602	10077.892757	28.032346
290.861479	10096.793860	28.037364
291.218791	10112.870314	28.042381
291.307329	10128.325408	28.047399
292.113564	10134.970329	28.052416
292.086352	10142.761334	28.057434
292.337674	10164.643415	28.062452
292.744995	10176.207646	28.067469
293.178859	10181.955354	28.072487
293.757476	10196.882645	28.077504
293.714012	10199.813073	28.082522
294.295538	10212.793692	28.087540
294.404337	10225.811105	28.092557
294.491153	10235.279555	28.097575
295.289665	10237.684267	28.102592
295.282109	10255.004630	28.107610
295.369392	10251.482145	28.112628
295.934873	10254.385571	28.117645
295.999174	10261.114960	28.122663
296.530392	10274.166218	28.127680
296.415158	10283.869946	28.132698
296.561693	10290.082565	28.137716
297.107095	10303.760789	28.142733
297.112082	10315.590724	28.147751
297.454444	10331.003998	28.152768
297.651588	10353.906673	28.157786
297.506200	10371.212149	28.162804
298.050492	10382.893221	28.167821
297.822636	10410.895003	28.172839
298.455046	10426.662730	28.177856
298.580328	10445.423994	28.182874
298.873967	10473.238104	28.187892
299.643868	10500.604891	28.192909
299.447131	10526.910655	28.197927
300.325722	10540.714642	28.202944
300.485576	10562.383255	28.207962
300.352873	10586.264769	28.212980
301.051122	10605.494870	28.217997
301.625232	10619.933782	28.223015
302.027200	10632.281902	28.228032
302.042695	10669.963007	28.233050
302.445399	10677.513020	28.238068
302.964857	10697.366127	28.243085
302.885578	10707.871481	28.248103
303.818438	10723.030887	28.253120
303.956159	10746.297393	28.258138
304.457288	10752.159344	28.263156
305.008826	10761.506051	28.268173
304.861233	10757.568741	28.273191
305.555134	10776.052088	28.278208
305.511954	10785.918979	28.283226
306.070119	10790.145873	28.288244
306.527240	10803.725295	28.293261
306.539856	10822.425496	28.298279
306.854916	10820.270230	28.303296
306.995077	10845.987286	28.308314
307.314669	10857.852110	28.313332
307.399232	10873.205896	28.318349
307.470500	10886.587958	28.323367
308.202222	10904.307138	28.328384
308.536760	10925.476216	28.333402
308.551870	10944.085269	28.338420
309.277373	10947.892025	28.343437
309.324089	10977.588066	28.348455
309.809148	10978.342092	28.353472
309.928225	10999.151706	28.358490
310.109105	11009.868049	28.363508
310.748061	11034.240778	28.368525
310.541497	11045.922410	28.373543
311.132946	11069.786474	28.378560
311.167148	11082.814155	28.383578
311.443104	11106.749809	28.388596
312.053264	11102.269003	28.393613
312.082050	11117.360793	28.398631
312.576509	11130.918426	28.403648
312.750576	11159.336448	28.408666
313.140524	11170.289540	28.413684
313.268636	11192.158516	28.418701
313.646849	11208.609019	28.423719
314.197265	11225.859278	28.428736
314.419996	11237.067311	28.433754
314.358297	11249.185251	28.438772
315.390768	11259.761722	28.443789
315.423693	11287.013255	28.448807
315.512353	11291.252944	28.453824
315.787828	11308.559315	28.458842
316.227961	11331.957188	28.463860
316.852633	11344.842193	28.468877
317.102748	11353.885894	28.473895
317.701597	11373.956472	28.478912
317.942577	11387.013245	28.483930
317.887086	11408.154651	28.488948
318.321492	11413.207784	28.493965
318.603603	11438.900473	28.498983
318.855861	11444.701620	28.504000
319.072227	11474.168145	28.509018
319.659193	11483.995273	28.514036
319.699845	11497.083674	28.519053
319.831559	11524.565058	28.524071
320.663547	11548.982629	28.529088
320.780978	11569.845433	28.534106
320.803264	11582.500607	28.539124
321.542953	11589.492083	28.544141
321.481895	11621.523673	28.549159
321.999621	11634.290007	28.554176
322.468723	11660.522319	28.559194
322.848465	11675.924915	28.564212
323.267834	11689.042852	28.569229
323.580998	11710.709144	28.574247
323.951208	11733.188469	28.579264
324.135256	11734.220729	28.584282
324.230527	11759.172805	28.589300
324.626068	11769.079033	28.594317
324.926641	11790.167375	28.599335
325.189340	11813.345951	28.604352
325.379324	11833.648769	28.609370
325.888859	11849.019249	28.614388
326.234140	11860.126949	28.619405
326.111933	11900.019166	28.624423
326.861232	11918.302063	28.629440
327.145791	11930.483819	28.634458
327.036770	11949.167018	28.639476
327.782914	11967.323167	28.644493
327.982413	11999.020841	28.649511
328.338334	12011.219625	28.654528
328.654175	12028.849980	28.659546
329.087077	12054.671395	28.664564
329.584955	12061.920835	28.669581
329.989554	12081.475896	28.674599
330.238951	12087.958578	28.679616
330.827548	12108.911341	28.684634
330.973441	12111.241912	28.689652
331.751079	12118.579813	28.694669
331.653193	12132.674899	28.699687
332.041141	12141.832094	28.704704
332.349651	12158.293956	28.709722
332.338306	12178.898901	28.714740
333.020846	12181.644353	28.719757
332.832888	12213.010284	28.724775
333.649969	12224.505679	28.729792
334.148477	12229.597478	28.734810
334.027364	12253.075794	28.739828
334.420934	12261.098354	28.744845
334.996551	12283.311995	28.749863
335.322544	12305.248250	28.754880
335.564080	12315.056398	28.759898
335.803434	12330.628240	28.764916
336.493470	12349.079117	28.769933
336.731475	12369.156187	28.774951
337.021854	12373.783363	28.779968
337.343353	12400.077476	28.784986
337.590364	12405.282813	28.790004
338.165451	12423.406561	28.795021
338.059815	12441.862942	28.800039
338.552115	12463.761314	28.805056
338.898530	12478.118270	28.810074
339.052742	12499.809647	28.815092
339.376242	12513.250158	28.820109
339.303920	12545.134367	28.825127
339.863895	12565.274714	28.830144
340.446279	12589.563539	28.835162
340.428583	12612.417686	28.840180
341.128688	12629.168905	28.845197
341.425996	12654.036142	28.850215
342.039706	12665.282302	28.855232
342.341744	12696.504040	28.860250
342.624722	12717.279072	28.865268
343.054999	12729.944763	28.870285
343.397095	12744.719441	28.875303
343.443434	12762.724388	28.880320
344.177186	12771.534049	28.885338
344.107716	12791.720893	28.890356
344.503389	12811.351917	28.895373
344.874581	12826.292057	28.900391
345.269690	12850.468086	28.905408
345.715273	12874.368486	28.910426
345.930264	12882.640429	28.915444
346.325876	12913.432097	28.920461
346.280202	12934.433166	28.925479
346.812607	12952.149532	28.930496
347.425317	12971.095218	28.935514
347.644022	13003.239415	28.940532
347.982185	12994.496578	28.945549
348.188956	13022.603145	28.950567
348.631421	13030.349517	28.955584
348.656695	13060.609952	28.960602
348.911325	13082.571692	28.965620
349.274671	13100.814613	28.970637
349.806370	13131.909142	28.975655
350.006465	13159.075014	28.980672
350.582252	13170.078071	28.985690
350.529708	13192.882361	28.990708
351.288334	13214.457678	28.995725
351.706155	13248.497594	29.000743
352.361454	13253.342587	29.005760
352.813636	13277.114363	29.010778
352.968891	13286.191657	29.015796
353.261299	13297.632852	29.020813
353.687946	13324.455337	29.025831
353.894785	13345.099116	29.030848
354.700553	13350.585601	29.035866
354.861766	13372.763371	29.040884
355.010767	13399.923449	29.045901
355.349830	13411.967932	29.050919
355.766950	13438.488196	29.055936
355.992679	13453.868837	29.060954
356.020986	13481.995639	29.065972
356.656033	13501.579473	29.070989
356.767205	13527.063447	29.076007
357.201071	13552.799295	29.081024
357.650573	13574.514049	29.086042
357.950552	13606.456960	29.091060
358.476371	13621.934099	29.096077
358.804480	13643.214863	29.101095
359.151673	13669.998174	29.106112
359.687685	13697.080874	29.111130
359.532911	13716.218082	29.116148
360.443392	13732.722695	29.121165
360.932287	13764.828296	29.126183
361.030761	13778.829949	29.131200
361.330728	13786.220491	29.136218
361.552771	13826.866796	29.141236
362.271683	13836.194264	29.146253
362.470203	13858.402415	29.151271
362.943835	13880.458422	29.156288
363.517156	13902.662112	29.161306
363.607931	13925.872688	29.166324
364.576164	13931.127062	29.171341
364.687031	13948.480490	29.176359
364.865278	13966.994530	29.181376
365.604932	13986.713756	29.186394
365.366030	13999.327544	29.191412
365.871564	14017.314624	29.196429
366.366395	14042.917506	29.201447
366.816846	14057.097022	29.206464
367.023988	14067.481021	29.211482
367.010890	14094.430238	29.216500
367.723257	14108.803238	29.221517
368.011160	14130.808616	29.226535
368.131376	14149.981954	29.231552
368.351350	14155.677608	29.236570
368.813304	14181.940416	29.241588
368.935361	14205.701601	29.246605
369.659147	14233.519604	29.251623
369.538108	14260.528526	29.256640
370.296785	14280.969131	29.261658
370.444377	14309.065261	29.266676
371.140372	14327.377089	29.271693
371.691596	14343.780505	29.276711
371.747565	14370.567272	29.281728
372.238631	14392.076890	29.286746
372.630083	14420.696013	29.291764
373.102708	14424.667966	29.296781
373.255113	14449.164669	29.301799
373.666410	14474.764662	29.306816
374.200671	14488.612406	29.311834
374.324430	14525.782785	29.316852
374.767553	14549.878880	29.321869
375.167240	14570.950172	29.326887
375.196243	14604.178804	29.331904
376.084720	14623.460083	29.336922
376.251845	14649.016717	29.341940
376.615493	14673.069484	29.346957
377.137755	14701.429490	29.351975
377.491076	14722.693573	29.356992
378.013899	14741.603346	29.362010
378.234693	14771.898006	29.367028
378.844240	14795.865631	29.372045
379.142445	14813.366036	29.377063
379.270345	14836.894939	29.382080
379.958098	14853.014509	29.387098
380.297402	14883.235497	29.392116
380.631380	14896.941451	29.397133
380.810422	14921.662765	29.402151
381.115049	14947.877862	29.407168
381.996388	14969.431399	29.412186
381.947816	14998.496566	29.417204
382.362762	15016.152482	29.422221
382.887168	15041.301239	29.427239
382.933731	15070.055479	29.432256
383.622950	15085.214628	29.437274
384.536373	15107.357616	29.442292
384.693128	15128.973994	29.447309
385.499294	15141.524238	29.452327
385.514481	15166.188411	29.457344
386.263245	15169.828134	29.462362
386.109182	15201.367294	29.467380
386.422914	15222.413228	29.472397
386.919048	15231.412170	29.477415
387.338925	15246.538233	29.482432
387.530053	15262.797893	29.487450
388.103181	15289.149890	29.492468
388.235892	15299.256878	29.497485
388.740508	15312.626231	29.502503
388.827739	15340.008021	29.507520
389.596597	15348.885836	29.512538
389.602116	15378.362710	29.517556
389.888614	15391.509848	29.522573
390.007670	15421.079519	29.527591
390.258920	15442.145453	29.532608
390.777384	15471.427898	29.537626
391.049970	15504.427572	29.542644
391.610737	15536.009983	29.547661
391.922696	15564.681429	29.552679
392.022364	15599.042588	29.557696
392.849522	15620.428741	29.562714
393.130512	15656.685222	29.567732
393.047780	15689.556803	29.572749
394.281133	15712.694109	29.577767
394.765363	15745.922445	29.582784
395.090514	15771.831693	29.587802
395.373188	15795.708899	29.592820
395.845296	15820.263132	29.597837
396.774555	15840.674124	29.602855
397.037605	15869.701222	29.607872
397.669237	15888.622338	29.612890
397.540696	15904.834121	29.617908
397.868737	15931.292111	29.622925
398.637001	15939.921980	29.627943
398.930434	15977.018251	29.632960
399.396249	15991.455940	29.637978
399.437019	16022.852858	29.642996
400.074193	16054.297112	29.648013
400.333691	16067.815912	29.653031
400.684255	16103.193385	29.658048
401.500636	16118.863152	29.663066
401.817456	16141.436615	29.668084
402.153803	16163.935160	29.673101
402.360030	16193.006956	29.678119
402.866126	16215.285640	29.683136
403.183315	16240.994218	29.688154
403.439520	16264.429380	29.693172
403.787520	16295.098259	29.698189
403.930146	16320.946975	29.703207
404.566162	16356.640724	29.708224
405.299862	16388.191724	29.713242
405.784940	16410.364210	29.718260
405.829316	16433.842829	29.723277
406.512359	16449.940040	29.728295
406.542360	16484.133780	29.733312
407.161971	16510.275669	29.738330
407.342051	16526.105304	29.743348
407.844557	16557.541930	29.748365
408.545738	16573.224615	29.753383
408.718156	16604.357080	29.758400
409.163598	16627.582542	29.763418
409.888398	16650.526938	29.768436
410.155498	16661.163451	29.773453
410.508902	16691.052022	29.778471
410.764954	16713.512003	29.783488
411.401351	16726.547552	29.788506
411.625712	16761.368354	29.793524
411.833588	16787.968211	29.798541
412.171794	16805.230480	29.803559
412.175881	16831.965629	29.808576
412.965582	16866.037987	29.813594
413.161679	16895.732943	29.818612
413.620916	16936.200876	29.823629
414.518299	16962.067010	29.828647
414.939595	16988.709777	29.833664
415.384587	17000.354712	29.838682
415.802876	17034.016972	29.843700
416.103409	17051.811464	29.848717
416.632185	17068.093146	29.853735
417.139423	17107.171895	29.858752
417.257485	17124.765639	29.863770
417.962438	17156.946768	29.868788
418.003351	17180.761301	29.873805
418.529464	17208.467989	29.878823
419.302493	17237.119180	29.883840
419.631700	17266.816867	29.888858
420.200455	17286.491019	29.893876
420.342511	17316.921925	29.898893
420.992806	17334.796244	29.903911
421.259680	17372.866385	29.908928
421.694908	17394.419722	29.913946
422.019195	17415.596692	29.918964
422.172729	17443.397414	29.923981
422.941408	17468.835718	29.928999
423.201608	17498.578111	29.934016
424.000628	17516.175807	29.939034
423.790978	17547.024995	29.944052
424.134645	17581.887097	29.949069
424.849749	17607.353850	29.954087
425.347043	17643.105750	29.959104
426.067659	17670.070098	29.964122
426.888245	17688.222409	29.969140
426.948871	17721.529190	29.974157
427.370297	17743.117889	29.979175
427.330295	17769.020563	29.984192
428.037622	17795.230576	29.989210
428.507662	17820.644997	29.994228
428.805648	17853.413074	29.999245
429.224653	17877.451107	30.004263
429.450882	17911.953144	30.009280
429.995104	17935.659118	30.014298
430.659062	17957.503958	30.019316
430.987264	17987.541567	30.024333
431.176051	18013.598744	30.029351
431.351108	18046.932478	30.034368
431.960411	18066.740140	30.039386
432.721479	18091.501164	30.044404
432.867782	18119.210943	30.049421
433.355912	18132.002217	30.054439
433.489167	18177.023140	30.059456
433.759129	18200.617705	30.064474
434.385955	18220.949938	30.069492
434.556094	18260.512472	30.074509
435.432790	18288.431381	30.079527
435.747605	18325.244641	30.084544
436.121875	18358.064228	30.089562
436.711341	18391.975595	30.094580
437.092526	18421.702450	30.099597
437.718288	18447.360415	30.104615
438.154958	18477.884454	30.109632
438.688540	18499.322872	30.114650
439.196174	18534.249968	30.119668
439.452285	18565.322642	30.124685
440.126228	18586.871105	30.129703
440.581798	18617.060116	30.134720
440.964615	18639.412140	30.139738
441.451264	18674.172023	30.144756
441.496655	18694.908941	30.149773
442.553337	18718.315958	30.154791
442.795839	18750.339231	30.159808
443.355934	18780.831997	30.164826
443.681703	18799.849915	30.169844
444.026504	18826.928913	30.174861
444.611030	18853.622114	30.179879
444.670380	18892.567659	30.184896
445.349743	18908.406407	30.189914
445.610734	18935.793449	30.194932
446.176189	18984.012956	30.199949
446.705244	19009.901050	30.204967
447.191409	19040.509652	30.209984
447.593422	19065.786157	30.215002
448.471157	19088.578116	30.220020
448.540542	19122.164071	30.225037
448.785608	19156.469791	30.230055
449.417420	19177.970274	30.235072
449.870274	19201.256888	30.240090
450.340618	19230.023780	30.245108
450.359639	19271.040213	30.250125
450.838745	19301.296491	30.255143
451.490465	19332.007253	30.260160
451.859832	19372.329507	30.265178
452.372510	19396.008092	30.270196
453.042631	19438.212274	30.275213
453.219095	19459.623473	30.280231
453.640503	19496.134700	30.285248
454.325483	19529.365955	30.290266
455.009876	19553.652121	30.295284
455.088911	19593.534152	30.300301
455.761852	19621.647388	30.305319
456.128174	19639.542055	30.310336
456.482453	19663.384878	30.315354
457.023566	19680.909194	30.320372
457.062212	19724.175473	30.325389
457.785159	19740.502272	30.330407
458.147146	19774.815135	30.335424
458.928844	19800.538692	30.340442
459.153448	19831.438575	30.345460
459.256758	19866.526784	30.350477
459.805303	19886.339759	30.355495
460.322868	19912.503655	30.360512
460.305766	19959.053046	30.365530
461.159610	19987.425162	30.370548
461.223284	20035.827477	30.375565
461.897091	20070.059418	30.380583
462.678516	20112.224459	30.385600
463.083491	20144.160920	30.390618
463.667576	20166.737040	30.395636
463.982029	20210.360771	30.400653
464.536081	20234.161613	30.405671
465.136168	20275.556276	30.410688
465.296135	20303.537476	30.415706
465.892986	20339.999492	30.420724
466.348373	20375.530849	30.425741
467.149681	20403.604177	30.430759
467.470440	20432.767247	30.435776
467.992162	20473.592946	30.440794
468.479220	20500.513188	30.445812
468.697173	20541.517791	30.450829
469.236094	20569.824192	30.455847
469.727874	20605.590860	30.460864
470.095363	20635.311121	30.465882
470.854754	20675.264315	30.470900
471.056561	20714.905588	30.475917
471.346173	20744.527421	30.480935
472.011989	20789.721065	30.485952
472.535950	20828.413517	30.490970
473.422478	20851.677214	30.495988
473.636544	20889.974230	30.501005
474.333570	20923.573131	30.506023
474.667698	20942.350160	30.511040
475.157858	20981.833552	30.516058
475.605836	21015.110055	30.521076
475.924141	21054.176045	30.526093
476.405573	21087.207958	30.531111
476.962793	21122.284941	30.536128
477.434298	21149.450553	30.541146
478.049090	21178.501620	30.546164
478.395900	21217.446916	30.551181
479.103368	21254.949547	30.556199
479.631128	21281.780380	30.561216
480.140556	21321.626982	30.566234
480.461193	21343.644289	30.571252
480.991482	21371.574304	30.576269
481.116328	21401.129903	30.581287
481.889533	21433.787652	30.586304
482.117477	21471.995667	30.591322
483.046876	21482.077522	30.596340
483.253178	21518.632061	30.601357
483.532021	21543.699466	30.606375
483.961232	21571.008007	30.611392
484.107623	21614.676980	30.616410
484.846461	21648.989827	30.621428
485.370387	21691.509656	30.626445
485.757445	21716.258456	30.631463
486.053705	21755.547069	30.636480
486.732661	21790.792807	30.641498
487.263075	21817.342966	30.646516
487.633828	21859.422188	30.651533
488.101662	21884.827044	30.656551
488.864973	21920.236841	30.661568
489.242707	21966.510714	30.666586
489.777696	22000.909572	30.671604
490.285218	22037.556732	30.676621
491.014885	22061.212661	30.681639
491.326397	22097.098864	30.686656
491.526882	22138.797193	30.691674
492.124122	22167.479564	30.696692
492.350841	22202.651773	30.701709
492.801881	22246.147945	30.706727
493.558469	22293.018497	30.711744
494.125706	22332.722192	30.716762
494.600784	22370.566944	30.721780
495.255153	22414.836915	30.726797
495.807570	22442.555802	30.731815
496.561444	22476.339570	30.736832
496.508131	22526.082305	30.741850
497.702012	22544.098923	30.746868
498.216238	22581.712687	30.751885
498.512062	22620.478967	30.756903
498.951530	22645.859638	30.761920
499.201776	22677.396638	30.766938
499.732592	22707.108970	30.771956
500.192853	22745.288572	30.776973
500.818982	22793.016276	30.781991
500.999226	22827.263935	30.787008
501.407585	22873.953031	30.792026
502.222515	22902.643806	30.797044
502.829249	22941.627567	30.802061
503.117725	22982.931311	30.807079
503.964210	23014.278698	30.812096
504.064052	23065.762258	30.817114
504.929743	23092.629774	30.822132
505.129530	23145.265748	30.827149
505.747152	23166.544375	30.832167
506.220284	23201.253432	30.837184
506.681413	23246.769497	30.842202
507.187760	23290.223498	30.847220
507.667798	23328.014615	30.852237
507.903372	23362.121500	30.857255
508.688978	23404.542031	30.862272
509.043936	23441.121441	30.867290
509.562503	23473.459293	30.872308
510.003644	23518.514600	30.877325
510.792004	23554.321847	30.882343
511.119753	23585.372555	30.887360
511.447102	23630.567607	30.892378
512.227510	23664.901061	30.897396
513.090653	23700.636076	30.902413
513.022748	23728.181918	30.907431
513.719303	23770.212746	30.912448
513.869604	23798.172928	30.917466
514.652002	23835.666609	30.922484
515.121793	23887.796513	30.927501
515.764693	23922.536032	30.932519
516.240992	23959.888145	30.937536
516.638742	24005.501551	30.942554
517.355020	24039.830278	30.947572
517.951397	24078.620774	30.952589
518.032107	24124.656026	30.957607
518.728464	24164.568240	30.962624
519.224207	24204.473911	30.967642
519.750533	24247.272769	30.972660
520.225034	24281.219898	30.977677
521.058793	24330.793104	30.982695
521.968919	24360.660012	30.987712
522.537277	24397.634568	30.992730
522.877732	24431.634091	30.997748
523.521135	24458.287269	31.002765
523.678624	24491.376322	31.007783
524.412913	24529.244016	31.012800
524.903421	24561.117499	31.017818
525.632551	24598.197674	31.022836
525.663930	24641.452959	31.027853
526.053840	24682.992306	31.032871
526.719763	24728.469751	31.037888
526.913892	24774.970901	31.042906
527.404661	24810.157238	31.047924
528.662909	24861.545584	31.052941
528.702587	24911.919809	31.057959
529.436143	24941.096731	31.062976
529.954326	24986.454289	31.067994
530.640227	25027.539337	31.073012
531.314971	25054.765937	31.078029
531.458514	25107.771836	31.083047
532.542207	25136.928008	31.088064
532.666795	25192.807756	31.093082
533.325511	25222.182235	31.098100
533.839620	25257.736085	31.103117
534.221489	25302.883079	31.108135
534.805972	25337.665715	31.113152
535.046098	25382.189550	31.118170
535.816371	25425.946865	31.123188
536.518033	25471.510540	31.128205
536.965869	25513.955837	31.133223
537.379159	25539.819537	31.138240
538.058824	25578.108851	31.143258
538.336659	25618.433259	31.148276
538.956381	25640.469555	31.153293
539.551431	25685.122038	31.158311
540.280343	25718.969470	31.163328
540.329454	25757.522717	31.168346
541.201379	25791.322314	31.173364
541.534692	25836.223305	31.178381
541.845017	25876.568398	31.183399
542.793550	25914.938587	31.188416
543.218492	25956.411062	31.193434
543.075261	26004.521455	31.198452
544.331925	26051.163521	31.203469
544.667533	26104.909432	31.208487
545.015524	26141.125878	31.213504
545.517393	26189.145102	31.218522
546.250125	26233.261175	31.223540
546.845211	26271.757054	31.228557
547.368906	26326.107140	31.233575
548.009065	26367.714202	31.238592
548.237190	26418.152949	31.243610
548.742509	26453.580078	31.248628
549.274158	26505.738602	31.253645
549.990248	26564.023914	31.258663
550.658908	26611.705860	31.263680
551.316282	26661.721695	31.268698
551.759715	26701.073122	31.273716
552.480468	26749.854860	31.278733
552.479070	26802.167000	31.283751
553.516241	26828.226483	31.288768
554.117568	26890.556277	31.293786
554.492071	26940.807901	31.298804
555.506770	26970.165133	31.303821
555.825294	27030.150216	31.308839
556.368680	27068.265470	31.313856
556.970729	27123.368399	31.318874
557.711674	27161.297991	31.323892
558.469585	27198.147983	31.328909
559.146750	27249.017306	31.333927
559.863364	27281.975788	31.338944
560.023699	27313.289660	31.343962
560.546430	27367.956195	31.348980
561.048129	27397.865478	31.353997
561.516778	27443.382836	31.359015
562.068140	27491.609998	31.364032
562.696020	27542.087861	31.369050
563.375574	27579.524772	31.374068
564.351379	27623.600431	31.379085
564.834856	27662.674439	31.384103
565.613781	27694.835973	31.389120
565.773050	27748.706057	31.394138
566.342235	27772.420477	31.399156
567.300253	27807.780850	31.404173
567.781654	27834.013215	31.409191
568.352078	27874.331341	31.414208
568.714503	27898.630393	31.419226
569.064847	27933.848310	31.424244
570.032960	27957.636558	31.429261
569.937575	28002.161195	31.434279
570.501133	28038.123812	31.439296
571.049725	28075.836433	31.444314
571.103883	28130.159442	31.449332
571.879259	28166.525103	31.454349
572.035281	28222.868118	31.459367
572.807132	28276.894522	31.464384
573.531090	28311.155550	31.469402
573.934891	28376.205343	31.474420
574.616544	28414.247390	31.479437
575.410313	28472.026117	31.484455
575.912371	28510.100145	31.489472
576.499310	28553.769108	31.494490
576.697199	28604.553570	31.499508
577.671445	28652.381191	31.504525
578.295531	28703.804060	31.509543
578.762844	28755.140175	31.514560
579.188313	28808.318982	31.519578
579.698437	28857.587390	31.524596
580.878389	28913.897373	31.529613
581.153124	28962.767075	31.534631
581.580809	29023.680586	31.539648
582.466383	29071.711096	31.544666
582.909190	29117.108053	31.549684
583.444171	29160.752256	31.554701
583.798402	29223.391200	31.559719
584.964054	29254.636964	31.564736
585.734277	29307.560785	31.569754
586.257315	29353.311233	31.574772
587.106784	29390.837165	31.579789
587.358267	29440.482623	31.584807
587.968210	29480.163359	31.589824
588.791249	29519.581745	31.594842
589.556055	29564.739560	31.599860
590.162970	29610.256743	31.604877
590.773821	29654.739615	31.609895
591.124502	29690.776048	31.614912
591.525291	29737.086014	31.619930
591.862632	29789.643808	31.624948
592.751608	29826.472615	31.629965
593.047318	29875.619083	31.634983
593.748186	29927.804238	31.640000
594.320801	29968.678806	31.645018
594.519216	30019.946690	31.650036
595.525589	30073.487845	31.655053
595.688381	30139.328502	31.660071
596.513699	30174.139949	31.665088
597.036314	30234.147708	31.670106
597.776507	30288.354475	31.675124
598.745864	30330.293603	31.680141
599.072782	30383.898280	31.685159
599.569700	30424.979895	31.690176
600.587716	30467.100747	31.695194
600.843510	30510.258759	31.700212
601.508810	30547.441599	31.705229
601.832988	30605.209704	31.710247
602.430400	30636.893778	31.715264
603.019051	30685.550013	31.720282
603.317652	30737.745083	31.725300
604.063757	30773.199263	31.730317
604.500225	30832.015689	31.735335
605.056954	30887.185103	31.740352
605.732279	30932.609973	31.745370
606.253491	30992.341775	31.750388
607.157147	31042.797628	31.755405
607.603647	31091.356350	31.760423
608.417733	31148.230369	31.765440
609.122042	31205.188264	31.770458
609.430814	31259.236846	31.775476
610.022845	31312.676255	31.780493
610.870490	31369.221022	31.785511
611.327685	31422.532533	31.790528
612.063845	31478.053625	31.795546
612.691503	31526.794409	31.800564
613.344625	31581.293569	31.805581
614.073919	31632.458312	31.810599
614.566934	31677.083662	31.815616
615.480659	31717.301471	31.820634
616.061368	31784.245362	31.825652
616.589425	31829.978300	31.830669
616.957355	31888.026082	31.835687
617.869354	31934.579235	31.840704
618.599395	31994.505241	31.845722
619.194518	32047.021343	31.850740
620.097770	32093.305241	31.855757
620.569220	32149.704550	31.860775
620.988600	32197.555279	31.865792
621.480975	32244.425170	31.870810
621.788293	32305.653776	31.875828
622.557572	32350.503335	31.880845
623.225756	32409.357858	31.885863
623.990628	32471.983234	31.890880
624.838106	32516.609582	31.895898
625.081786	32575.740359	31.900916
625.978941	32628.862771	31.905933
626.599856	32690.391210	31.910951
627.520202	32735.490449	31.915968
628.364811	32782.036243	31.920986
628.460667	32842.217641	31.926004
629.561266	32879.043268	31.931021
630.386098	32926.015052	31.936039
630.265617	32986.344913	31.941056
631.225552	33030.625310	31.946074
631.767449	33088.745764	31.951092
632.415579	33136.181332	31.956109
632.903277	33191.440398	31.961127
633.479685	33239.161954	31.966144
634.311593	33269.292663	31.971162
634.867804	33320.526467	31.976180
635.896377	33363.099170	31.981197
635.968990	33405.542052	31.986215
636.595573	33443.779545	31.991232
637.506731	33478.275390	31.996250
637.684257	33531.747019	32.001268
638.348665	33584.130876	32.006285
638.748768	33644.038173	32.011303
639.183160	33695.108107	32.016320
639.826985	33756.517064	32.021338
640.410120	33816.268155	32.026356
641.315807	33872.646759	32.031373
642.106654	33934.274143	32.036391
642.411006	33997.617050	32.041408
643.030433	34045.513783	32.046426
643.781763	34115.294724	32.051444
645.035688	34168.847644	32.056461
645.347232	34223.769332	32.061479
645.778666	34279.356256	32.066496
646.625438	34333.901451	32.071514
646.824727	34404.928577	32.076532
648.140321	34446.394304	32.081549
648.646267	34511.058032	32.086567
649.165005	34569.893591	32.091584
650.174494	34623.080190	32.096602
650.690002	34680.660258	32.101620
651.464782	34727.303042	32.106637
652.107938	34791.056911	32.111655
652.653406	34845.141001	32.116672
653.498990	34891.700456	32.121690
653.913400	34958.344732	32.126708
654.581847	35009.669923	32.131725
655.401142	35062.818851	32.136743
655.736226	35115.378209	32.141760
656.623484	35171.515077	32.146778
657.231552	35239.195325	32.151796
658.218466	35288.495354	32.156813
658.823754	35345.615707	32.161831
659.281819	35396.655564	32.166848
660.274167	35457.458809	32.171866
660.572680	35514.939156	32.176884
661.315894	35568.844339	32.181901
661.781404	35625.866516	32.186919
662.529230	35681.420349	32.191936
663.372299	35742.981480	32.196954
664.155908	35799.773878	32.201972
664.842689	35851.741960	32.206989
665.474483	35900.786617	32.212007
665.985282	35966.833099	32.217024
666.904914	36003.598328	32.222042
667.414251	36066.940099	32.227060
667.985062	36122.157824	32.232077
668.713146	36176.877724	32.237095
669.331668	36227.579257	32.242112
670.055920	36286.886335	32.247130
670.570039	36333.147866	32.252148
671.121224	36378.695742	32.257165
671.913102	36435.356549	32.262183
672.132213	36492.441405	32.267200
672.858614	36541.124450	32.272218
673.241732	36599.837397	32.277236
674.117031	36654.570102	32.282253
674.862095	36715.653786	32.287271
675.153325	36784.226328	32.292288
675.973230	36837.890049	32.297306
676.691683	36906.043479	32.302324
677.575629	36963.728828	32.307341
678.023305	37038.011690	32.312359
678.601165	37101.106804	32.317376
679.314613	37157.151879	32.322394
679.821999	37228.460404	32.327412
680.468049	37295.452333	32.332429
681.330928	37361.686317	32.337447
682.328350	37429.857365	32.342464
683.083298	37493.293117	32.347482
683.958511	37565.512582	32.352500
684.676630	37623.152493	32.357517
685.098575	37684.708966	32.362535
685.667836	37752.258898	32.367552
686.969306	37805.882145	32.372570
687.325766	37865.623879	32.377588
688.102815	37928.892198	32.382605
689.125711	37983.194205	32.387623
689.466651	38045.513834	32.392640
690.280801	38106.809155	32.397658
690.705252	38170.760483	32.402676
691.650627	38226.713850	32.407693
692.459192	38295.262198	32.412711
692.783267	38359.734782	32.417728
693.801793	38415.787502	32.422746
694.302105	38468.332615	32.427764
695.383421	38537.713626	32.432781
695.970365	38593.334236	32.437799
696.556994	38651.900512	32.442816
697.697515	38705.547519	32.447834
698.107768	38770.100974	32.452852
698.814408	38820.613377	32.457869
699.776540	38874.686677	32.462887
700.654698	38927.835317	32.467904
701.654465	38977.901011	32.472922
702.138077	39034.846702	32.477940
702.588014	39087.360759	32.482957
703.469239	39133.428036	32.487975
703.818084	39198.623631	32.492992
704.399532	39241.681446	32.498010
704.777083	39302.823547	32.503028
705.446008	39368.634263	32.508045
706.428864	39434.521401	32.513063
706.755603	39492.553251	32.518080
707.556744	39545.386525	32.523098
708.485567	39606.894512	32.528116
708.922488	39653.283085	32.533133
709.732027	39719.295111	32.538151
710.298341	39773.000652	32.543168
710.768997	39823.749147	32.548186
711.361385	39888.487580	32.553204
712.206249	39960.162294	32.558221
713.227394	40012.487346	32.563239
713.616266	40078.704931	32.568256
714.227598	40149.274356	32.573274
714.959157	40204.076140	32.578292
715.603706	40279.789489	32.583309
716.309638	40332.758637	32.588327
717.048595	40404.718584	32.593344
717.734599	40475.569206	32.598362
718.533268	40548.278767	32.603380
719.175534	40617.619905	32.608397
720.165756	40689.769712	32.613415
720.974852	40766.427284	32.618432
721.568034	40822.643982	32.623450
722.848222	40889.355179	32.628468
723.441132	40950.927807	32.633485
724.233974	41010.336719	32.638503
724.886919	41079.567641	32.643520
725.993600	41128.796297	32.648538
726.651751	41187.687930	32.653556
727.153423	41261.182697	32.658573
727.867247	41316.470290	32.663591
728.796932	41392.928536	32.668608
729.122864	41447.347852	32.673626
730.236504	41515.056312	32.678644
730.584307	41580.105036	32.683661
731.160211	41626.823794	32.688679
731.650512	41709.563862	32.693696
732.972998	41778.293595	32.698714
733.564346	41846.007657	32.703732
734.541440	41914.184169	32.708749
735.451572	41971.653698	32.713767
736.238138	42038.839081	32.718784
736.689294	42086.001611	32.723802
737.892446	42151.326375	32.728820
738.252025	42218.290247	32.733837
739.029637	42276.264489	32.738855
739.723128	42339.658701	32.743872
740.813682	42393.795268	32.748890
741.180552	42459.588688	32.753908
741.910039	42527.018482	32.758925
742.972945	42584.241785	32.763943
743.279588	42656.852513	32.768960
744.200306	42711.323085	32.773978
745.094973	42788.632166	32.778996
746.021309	42840.774357	32.784013
746.255034	42895.048904	32.789031
747.074388	42951.495224	32.794048
747.758302	43013.442434	32.799066
748.540850	43062.179384	32.804084
748.810885	43131.719260	32.809101
750.210916	43182.478003	32.814119
750.367469	43252.597914	32.819136
751.187064	43308.720460	32.824154
752.047279	43372.347437	32.829172
752.368466	43435.287616	32.834189
753.055816	43510.566769	32.839207
753.457974	43581.516390	32.844224
754.121170	43652.099834	32.849242
755.076097	43720.205006	32.854260
755.863236	43800.276992	32.859277
756.825795	43869.785297	32.864295
757.506811	43952.234466	32.869312
758.386172	44019.592599	32.874330
759.420757	44104.528780	32.879348
759.853637	44183.829280	32.884365
760.823432	44239.337872	32.889383
761.715532	44308.392272	32.894400
762.401148	44388.845917	32.899418
763.367134	44459.403375	32.904436
763.703092	44530.837455	32.909453
764.640703	44592.617433	32.914471
765.400285	44681.862160	32.919488
766.338281	44756.024763	32.924506
767.408297	44830.535768	32.929524
767.851576	44886.111314	32.934541
768.579050	44958.683616	32.939559
769.129478	45042.423789	32.944576
769.966808	45113.789913	32.949594
770.991020	45189.312956	32.954612
771.572387	45269.351906	32.959629
772.529067	45337.472607	32.964647
773.570193	45423.777062	32.969664
774.041421	45493.146081	32.974682
775.074925	45560.192248	32.979700
775.739238	45643.443950	32.984717
776.734254	45707.786796	32.989735
777.374931	45781.855969	32.994752
778.316227	45864.723909	32.999770
778.727876	45936.839460	33.004788
779.586114	46006.221472	33.009805
780.566115	46078.562628	33.014823
781.417274	46154.991312	33.019840
781.880239	46215.347690	33.024858
782.717890	46287.592482	33.029876
783.810701	46364.160290	33.034893
784.566152	46424.085923	33.039911
785.091198	46513.718081	33.044928
785.757359	46575.141296	33.049946
786.853053	46648.614818	33.054964
787.328890	46732.046827	33.059981
788.035879	46805.620740	33.064999
789.014125	46869.008233	33.070016
789.949413	46935.217126	33.075034
790.711269	46986.729063	33.080052
791.287385	47066.852785	33.085069
792.206659	47119.119364	33.090087
792.770853	47188.953561	33.095104
793.160319	47264.542425	33.100122
794.419261	47331.262909	33.105140
794.891279	47417.443758	33.110157
795.825740	47481.272689	33.115175
796.605697	47552.279261	33.120192
797.345521	47639.702732	33.125210
797.978897	47702.185786	33.130228
798.761706	47785.542373	33.135245
799.412827	47855.684054	33.140263
800.073297	47943.115348	33.145280
800.511357	48036.381875	33.150298
801.673112	48111.715765	33.155316
802.380454	48209.550224	33.160333
803.355192	48292.610453	33.165351
804.376430	48370.596198	33.170368
804.872466	48469.784661	33.175386
805.932719	48546.029525	33.180404
806.773970	48636.505645	33.185421
807.867009	48706.886437	33.190439
808.932596	48796.056040	33.195456
809.662943	48867.735277	33.200474
810.687128	48943.186116	33.205492
811.247141	49013.936957	33.210509
812.074285	49093.774323	33.215527
812.874414	49173.231379	33.220544
813.543771	49257.796261	33.225562
814.834288	49335.579311	33.230580
815.622738	49424.124061	33.235597
816.487845	49489.659489	33.240615
817.210456	49573.128736	33.245632
817.589765	49650.663754	33.250650
819.012402	49731.245429	33.255668
819.704513	49813.458426	33.260685
820.644577	49878.951804	33.265703
821.603258	49952.637597	33.270720
822.581663	50045.793965	33.275738
823.457486	50111.819104	33.280756
824.053211	50191.464713	33.285773
824.682550	50246.090316	33.290791
825.851511	50318.251522	33.295808
826.698644	50401.259880	33.300826
827.744171	50460.626028	33.305844
828.107081	50536.539161	33.310861
829.016134	50620.125644	33.315879
829.846489	50681.095173	33.320896
830.450702	50761.499352	33.325914
831.624894	50838.152477	33.330932
832.121017	50904.080036	33.335949
833.106939	50972.404028	33.340967
833.809084	51043.238134	33.345984
834.283231	51111.634642	33.351002
835.680161	51176.555140	33.356020
836.109049	51250.617793	33.361037
836.660141	51322.114523	33.366055
837.392850	51392.317129	33.371072
838.169801	51472.602331	33.376090
839.112209	51540.925951	33.381108
839.644157	51621.708418	33.386125
840.320539	51705.109771	33.391143
841.386806	51798.614749	33.396160
842.113218	51879.635681	33.401178
842.898235	51962.550702	33.406196
843.316397	52050.438362	33.411213
844.218057	52144.782426	33.416231
845.376107	52234.989666	33.421248
845.920798	52327.352711	33.426266
847.096285	52412.139152	33.431284
848.364660	52496.238968	33.436301
849.578271	52578.201760	33.441319
849.976749	52677.444873	33.446336
850.632950	52748.946324	33.451354
851.808533	52830.569144	33.456372
852.640879	52922.068860	33.461389
853.312458	53008.541623	33.466407
854.351743	53091.894795	33.471424
855.021248	53180.290816	33.476442
855.873345	53273.979562	33.481460
856.788801	53368.539295	33.486477
857.668962	53457.360795	33.491495
858.827282	53544.882276	33.496512
859.552322	53640.483732	33.501530
860.772792	53710.987026	33.506548
861.731952	53804.165941	33.511565
862.418243	53898.657597	33.516583
863.352082	53969.141230	33.521600
864.191474	54059.957498	33.526618
865.277889	54132.506980	33.531636
866.584827	54206.587213	33.536653
867.416604	54277.508083	33.541671
868.428331	54348.501598	33.546688
869.223618	54431.539937	33.551706
870.410835	54498.888876	33.556724
871.165595	54563.756496	33.561741
871.713732	54655.401727	33.566759
872.387604	54724.370382	33.571776
873.018992	54800.949982	33.576794
874.010732	54885.019700	33.581812
874.584294	54973.332396	33.586829
875.223396	55056.751969	33.591847
876.099048	55136.564250	33.596864
877.157819	55228.942327	33.601882
878.050943	55321.176777	33.606900
878.828595	55411.286759	33.611917
879.848755	55493.091494	33.616935
880.799881	55572.139246	33.621952
881.496202	55661.474253	33.626970
881.955805	55733.684782	33.631988
882.555247	55808.761667	33.637005
883.462100	55902.471015	33.642023
884.234531	55991.287298	33.647040
884.837034	56098.768134	33.652058
885.593269	56175.731367	33.657076
886.661240	56272.191707	33.662093
887.137599	56380.754925	33.667111
888.490095	56463.912703	33.672128
889.601901	56567.429274	33.677146
890.351766	56667.664145	33.682164
891.255541	56772.297752	33.687181
892.021053	56860.566899	33.692199
893.696292	56944.793012	33.697216
894.201050	57059.126406	33.702234
895.072270	57134.137048	33.707252
896.199700	57227.650742	33.712269
896.946113	57317.134203	33.717287
898.010235	57418.342829	33.722304
898.799608	57507.552039	33.727322
899.945840	57609.042241	33.732340
900.827315	57699.434205	33.737357
901.864285	57793.078812	33.742375
903.122996	57877.246040	33.747392
903.354871	57979.256300	33.752410
904.572655	58073.615454	33.757428
905.649701	58154.109659	33.762445
906.395785	58257.760215	33.767463
907.556455	58337.481060	33.772480
908.368943	58442.991072	33.777498
909.549741	58515.697588	33.782516
910.390722	58616.323174	33.787533
911.195520	58705.737762	33.792551
912.239891	58796.327004	33.797568
913.150376	58894.745663	33.802586
913.844597	58990.019973	33.807604
914.909641	59071.539843	33.812621
915.597696	59159.507096	33.817639
916.407942	59259.238091	33.822656
917.458392	59347.473761	33.827674
918.344840	59439.783551	33.832692
919.124833	59549.579943	33.837709
920.138407	59649.899502	33.842727
921.346196	59723.853586	33.847744
922.166534	59836.130046	33.852762
923.076855	59913.308485	33.857780
924.117863	60012.233242	33.862797
925.266751	60102.035500	33.867815
926.213983	60192.457551	33.872832
926.679212	60288.510603	33.877850
928.040363	60368.467165	33.882868
928.869230	60472.211597	33.887885
929.232549	60553.552807	33.892903
930.776773	60640.743532	33.897920
931.484414	60732.507190	33.902938
932.100716	60809.578239	33.907956
932.969831	60896.830215	33.912973
933.914595	60984.910461	33.917991
934.706577	61066.820351	33.923008
935.739265	61166.156695	33.928026
936.468411	61243.284193	33.933044
937.306202	61337.300386	33.938061
938.288862	61445.181101	33.943079
939.422639	61518.569906	33.948096
940.307627	61633.707640	33.953114
940.983058	61720.034339	33.958132
942.046796	61818.090342	33.963149
942.951980	61910.684046	33.968167
943.888652	62019.784759	33.973184
944.517908	62125.480482	33.978202
945.789293	62224.443400	33.983220
946.730869	62325.530794	33.988237
947.401470	62420.466318	33.993255
948.513415	62526.444311	33.998272
949.571777	62631.509347	34.003290
950.191750	62727.856530	34.008308
951.389173	62841.423538	34.013325
952.260215	62945.105412	34.018343
953.303411	63053.443574	34.023360
954.216949	63169.318748	34.028378
955.621364	63260.743848	34.033396
956.560971	63364.312895	34.038413
957.298217	63478.136936	34.043431
958.475821	63576.149202	34.048448
958.955077	63686.342840	34.053466
960.261089	63789.255892	34.058484
961.368399	63904.905769	34.063501
962.289124	64005.045401	34.068519
963.270335	64108.021330	34.073536
964.145613	64215.296994	34.078554
965.313916	64313.917731	34.083572
966.884397	64421.282905	34.088589
967.145875	64523.740813	34.093607
968.449017	64621.871132	34.098624
969.636048	64715.643247	34.103642
970.475273	64822.040621	34.108660
971.586151	64933.660045	34.113677
972.534970	65021.609988	34.118695
973.539394	65117.945999	34.123712
974.542491	65219.392710	34.128730
975.417351	65319.398095	34.133748
976.682092	65411.623199	34.138765
977.276554	65519.051920	34.143783
978.373040	65611.816396	34.148800
979.572948	65715.246248	34.153818
980.104511	65815.488860	34.158836
981.309223	65911.048470	34.163853
982.350952	66013.961863	34.168871
983.163539	66087.984774	34.173888
983.900245	66194.851402	34.178906
984.884071	66271.282888	34.183924
986.151421	66364.023814	34.188941
986.524701	66454.020626	34.193959
987.437311	66556.865870	34.198976
988.709338	66641.325954	34.203994
989.414927	66750.310461	34.209012
990.335279	66840.841103	34.214029
991.251825	66953.207520	34.219047
991.909670	67047.473187	34.224064
993.043485	67158.605994	34.229082
994.273936	67269.092355	34.234100
995.215074	67376.359406	34.239117
996.121075	67489.318110	34.244135
997.660960	67598.550542	34.249152
998.449029	67705.553176	34.254170
999.757804	67809.858202	34.259188
1000.446881	67895.784205	34.264205
1001.161952	68012.743610	34.269223
1002.398638	68115.760374	34.274240
1003.474738	68229.871364	34.279258
1004.752425	68331.947773	34.284276
1005.840514	68429.777937	34.289293
1006.751281	68543.051570	34.294311
1007.745265	68646.368776	34.299328
1008.941629	68758.694818	34.304346
1009.953479	68856.589796	34.309364
1011.219809	68976.594524	34.314381
1011.824026	69068.894783	34.319399
1013.103229	69162.629626	34.324416
1013.939792	69272.905745	34.329434
1014.767332	69383.891516	34.334452
1016.330363	69476.938302	34.339469
1017.130811	69599.345931	34.344487
1018.370885	69694.384715	34.349504
1019.477412	69805.233726	34.354522
1020.534197	69898.186148	34.359540
1021.584394	69998.045633	34.364557
1022.213002	70103.507288	34.369575
1023.545816	70203.278633	34.374592
1024.187093	70323.536370	34.379610
1025.145355	70428.069110	34.384628
1026.578759	70533.626185	34.389645
1027.567861	70636.556631	34.394663
1028.724288	70743.586809	34.399680
1029.317392	70850.391265	34.404698
1030.564221	70957.003853	34.409716
1031.542890	71065.289807	34.414733
1032.373912	71176.127193	34.419751
1033.842045	71285.410620	34.424768
1034.598385	71380.307049	34.429786
1035.686838	71484.167566	34.434804
1037.125261	71590.336082	34.439821
1037.798661	71683.661215	34.444839
1039.060629	71781.676321	34.449856
1040.243671	71872.640273	34.454874
1040.966374	71955.545797	34.459892
1042.374650	72050.025805	34.464909
1042.658420	72151.123881	34.469927
1044.023394	72232.159164	34.474944
1044.857207	72329.632176	34.479962
1045.713134	72439.328984	34.484980
1047.046019	72527.637179	34.489997
1047.455594	72643.269967	34.495015
1048.689131	72748.674792	34.500032
1049.805047	72846.952199	34.505050
1050.702642	72960.916840	34.510068
1051.746810	73069.070632	34.515085
1052.637879	73181.824331	34.520103
1053.775825	73299.297644	34.525120
1054.800060	73414.211548	34.530138
1055.543573	73533.069667	34.535156
1057.161462	73642.639265	34.540173
1057.957811	73761.793661	34.545191
1058.965111	73880.175861	34.550208
1059.864614	73995.681681	34.555226
1060.666025	74113.990585	34.560244
1062.317578	74230.123814	34.565261
1063.308560	74346.097375	34.570279
1064.357368	74469.013770	34.575296
1065.976935	74580.540944	34.580314
1066.842879	74698.154209	34.585332
1068.150825	74803.583323	34.590349
1069.247555	74926.874072	34.595367
1070.124606	75044.380163	34.600384
1071.593363	75146.600421	34.605402
1072.626237	75265.959953	34.610420
1073.935974	75382.982102	34.615437
1074.440614	75488.833286	34.620455
1075.471386	75606.469879	34.625472
1076.590698	75712.951246	34.630490
1077.391048	75836.130384	34.635508
1078.760563	75949.796793	34.640525
1079.747759	76073.567008	34.645543
1080.675115	76187.279800	34.650560
1081.929907	76317.227783	34.655578
1083.326945	76425.116009	34.660596
1084.816732	76541.446309	34.665613
1085.340523	76650.492158	34.670631
1086.574636	76771.674044	34.675648
1087.844599	76886.145244	34.680666
1088.843871	77010.273187	34.685684
1089.888060	77110.858134	34.690701
1091.184825	77234.219620	34.695719
1092.269415	77345.935649	34.700736
1093.382671	77458.734832	34.705754
1094.009343	77578.842555	34.710772
1095.624633	77687.549711	34.715789
1096.401684	77798.015123	34.720807
1097.684226	77913.362325	34.725824
1098.537575	78006.523865	34.730842
1099.583989	78103.245198	34.735860
1100.490844	78217.964931	34.740877
1101.605788	78321.521597	34.745895
1102.543317	78432.438961	34.750912
1103.815373	78534.100802	34.755930
1104.788609	78649.665689	34.760948
1106.047132	78750.850384	34.765965
1107.203690	78874.263041	34.770983
1108.161313	78978.290504	34.776000
1109.437353	79096.875352	34.781018
1110.302797	79205.216808	34.786036
1111.366206	79318.994953	34.791053
1112.762614	79432.670199	34.796071
1113.827755	79561.164612	34.801088
1114.854043	79673.743311	34.806106
1115.772849	79790.928815	34.811124
1117.276402	79916.669266	34.816141
1118.396576	80021.807631	34.821159
1119.356255	80142.635932	34.826176
1120.721202	80252.186653	34.831194
1121.610549	80361.529137	34.836212
1123.139037	80494.108729	34.841229
1124.169610	80608.967509	34.846247
1125.102929	80720.966176	34.851264
1126.697361	80837.158853	34.856282
1127.524670	80965.756717	34.861300
1129.112545	81062.873636	34.866317
1130.096811	81196.656852	34.871335
1131.385205	81297.488969	34.876352
1132.312494	81408.196390	34.881370
1133.603695	81525.212378	34.886388
1134.144308	81641.261069	34.891405
1135.457659	81756.896720	34.896423
1137.062766	81878.138221	34.901440
1138.012055	81999.478401	34.906458
1138.838456	82118.442874	34.911476
1140.224325	82228.771961	34.916493
1141.451800	82362.707320	34.921511
1142.448654	82483.138721	34.926528
1144.051478	82583.244296	34.931546
1144.981409	82712.974565	34.936564
1145.783374	82830.701550	34.941581
1146.903535	82949.857950	34.946599
1148.348460	83076.581473	34.951616
1149.565015	83194.415265	34.956634
1150.406112	83309.167324	34.961652
1151.720787	83429.863408	34.966669
1153.128759	83555.154241	34.971687
1153.948728	83668.564990	34.976704
1155.335657	83785.584724	34.981722
1156.307349	83913.393792	34.986740
1157.361330	84031.555278	34.991757
1158.892217	84142.004143	34.996775
1159.899726	84252.075278	35.001792
1161.049202	84364.115984	35.006810
1161.792687	84477.853047	35.011828
1163.074865	84569.433146	35.016845
1164.387329	84683.788960	35.021863
1165.335455	84803.507978	35.026880
1166.558077	84906.840054	35.031898
1167.411365	85023.711252	35.036916
1168.391336	85140.980247	35.041933
1169.659293	85265.962075	35.046951
1170.874506	85377.491874	35.051968
1172.382500	85493.193004	35.056986
1172.984406	85630.447942	35.062004
1174.008169	85746.992516	35.067021
1175.613996	85883.362317	35.072039
1176.465987	86004.152991	35.077056
1177.871137	86119.924468	35.082074
1179.000020	86250.435186	35.087092
1180.162887	86382.661169	35.092109
1181.512733	86506.834235	35.097127
1182.314798	86637.772349	35.102144
1183.878373	86769.051768	35.107162
1184.662088	86901.840781	35.112180
1186.455537	87020.109972	35.117197
1187.681591	87153.196954	35.122215
1188.852733	87289.094726	35.127232
1190.010878	87407.587218	35.132250
1191.090036	87543.096529	35.137268
1192.697804	87662.638177	35.142285
1193.893030	87792.426870	35.147303
1194.945170	87920.677191	35.152320
1196.235049	88034.510740	35.157338
1197.549065	88171.795198	35.162356
1198.916099	88291.865537	35.167373
1199.863165	88431.543410	35.172391
1201.024727	88554.297491	35.177408
1202.350261	88675.445267	35.182426
1203.493263	88818.932991	35.187444
1204.745979	88940.340456	35.192461
1206.103682	89064.773676	35.197479
1207.304422	89190.737652	35.202496
1208.679513	89312.374376	35.207514
1209.526360	89451.834455	35.212532
1210.847440	89574.303350	35.217549
1212.622384	89685.918312	35.222567
1213.335441	89827.071613	35.227584
1214.631134	89949.091323	35.232602
1216.000090	90075.817874	35.237620
1217.258848	90203.112885	35.242637
1218.390011	90326.394083	35.247655
1219.603279	90443.458842	35.252672
1221.126496	90552.462095	35.257690
1222.394217	90684.198128	35.262708
1223.614942	90814.152638	35.267725
1224.957980	90928.328110	35.272743
1225.942176	91029.387481	35.277760
1226.862409	91146.319188	35.282778
1228.081983	91257.050209	35.287796
1229.214762	91374.942285	35.292813
1230.349756	91485.162972	35.297831
1231.071185	91606.372505	35.302848
1232.548267	91715.572299	35.307866
1233.511460	91855.351769	35.312884
1234.736556	91967.097437	35.317901
1235.993173	92094.214040	35.322919
1236.681320	92228.777444	35.327936
1237.791792	92365.121364	35.332954
1239.436414	92495.948172	35.337972
1240.208833	92638.988601	35.342989
1241.579467	92774.743423	35.348007
1242.826610	92922.510818	35.353024
1244.314149	93060.013466	35.358042
1245.485093	93203.848058	35.363060
1246.881991	93344.453499	35.368077
1248.095381	93495.177562	35.373095
1248.983891	93630.729647	35.378112
1250.243396	93773.497549	35.383130
1251.499693	93922.383380	35.388148
1252.921618	94075.918256	35.393165
1254.699380	94217.588243	35.398183
1256.060403	94358.250074	35.403200
1257.491212	94495.928759	35.408218
1258.626632	94638.702954	35.413236
1259.667470	94777.508046	35.418253
1261.191277	94906.166995	35.423271
1262.557747	95057.870390	35.428288
1263.690943	95198.516797	35.433306
1265.252355	95335.256348	35.438324
1266.528897	95466.083237	35.443341
1267.767089	95615.426018	35.448359
1268.996076	95760.786028	35.453376
1270.293150	95897.697542	35.458394
1271.729165	96026.503390	35.463412
1273.032180	96157.551497	35.468429
1274.526859	96302.739925	35.473447
1275.749004	96448.668467	35.478464
1276.917881	96579.386097	35.483482
1278.268499	96712.049309	35.488500
1279.446598	96840.590832	35.493517
1281.039379	96981.478960	35.498535
1282.483755	97128.135691	35.503552
1283.676295	97263.332415	35.508570
1284.817762	97394.223587	35.513588
1286.313055	97510.844192	35.518605
1287.663650	97649.269779	35.523623
1288.758871	97787.148457	35.528640
1290.199689	97918.906054	35.533658
1291.399487	98061.172913	35.538676
1292.522427	98171.959900	35.543693
1293.873854	98307.991644	35.548711
1294.908676	98445.232278	35.553728
1296.344312	98563.284897	35.558746
1297.500796	98688.936425	35.563764
1298.327638	98811.389169	35.568781
1299.782811	98923.423943	35.573799
1301.028270	99057.319609	35.578816
1301.926891	99188.057224	35.583834
1303.112132	99329.030983	35.588852
1304.112858	99463.575291	35.593869
1305.599671	99600.206890	35.598887
1306.413525	99749.853070	35.603904
1307.863757	99900.474638	35.608922
1309.508851	100053.666590	35.613940
1310.321959	100212.534253	35.618957
1311.798563	100356.081032	35.623975
1312.759640	100509.327795	35.628992
1314.415703	100661.478071	35.634010
1315.798464	100831.509043	35.639028
1317.148828	100985.019760	35.644045
1318.748483	101133.569275	35.649063
1319.891412	101290.607625	35.654080
1321.334791	101446.283194	35.659098
1322.923557	101597.172190	35.664116
1324.071442	101762.242366	35.669133
1325.726285	101900.993186	35.674151
1326.973682	102067.030457	35.679168
1328.221337	102215.978194	35.684186
1329.800969	102357.312664	35.689204
1331.335932	102524.250286	35.694221
1333.226708	102673.491029	35.699239
1333.877801	102818.633263	35.704256
1335.452222	102960.541699	35.709274
1336.982421	103113.753101	35.714292
1337.986022	103270.377637	35.719309
1339.793478	103406.683253	35.724327
1340.901536	103564.843471	35.729344
1342.327414	103703.445207	35.734362
1343.737178	103859.673726	35.739380
1345.525613	103998.915652	35.744397
1346.735527	104152.077147	35.749415
1348.017998	104290.692472	35.754432
1349.227852	104439.647660	35.759450
1351.168229	104576.698296	35.764468
1351.928092	104729.979362	35.769485
1353.480486	104872.168599	35.774503
1354.409839	105028.784954	35.779520
1355.877593	105174.780103	35.784538
1357.382776	105316.732702	35.789556
1358.183973	105473.100234	35.794573
1359.939826	105629.817007	35.799591
1361.518381	105777.734751	35.804608
1362.610623	105927.338151	35.809626
1364.240936	106070.591690	35.814644
1365.606372	106236.766095	35.819661
1366.930527	106370.127849	35.824679
1367.910175	106523.170340	35.829696
1369.242941	106649.716290	35.834714
1370.648804	106786.934225	35.839732
1371.889333	106932.495252	35.844749
1373.202039	107051.097548	35.849767
1374.522404	107214.482225	35.854784
1375.366024	107356.925484	35.859802
1377.182293	107498.664384	35.864820
1378.342932	107652.014401	35.869837
1379.842642	107792.147146	35.874855
1381.208363	107944.529735	35.879872
1382.536744	108097.140737	35.884890
1384.146799	108246.087670	35.889908
1385.114041	108401.416223	35.894925
1386.820723	108557.640929	35.899943
1388.252752	108715.606533	35.904960
1389.918781	108856.674729	35.909978
1391.408406	109009.202556	35.914996
1392.580450	109167.782058	35.920013
1394.178929	109310.306721	35.925031
1395.785766	109455.685472	35.930048
1396.885292	109618.887274	35.935066
1398.128174	109777.396187	35.940084
1399.493797	109927.759451	35.945101
1401.328908	110092.904629	35.950119
1402.358896	110245.070155	35.955136
1403.702573	110406.453447	35.960154
1405.694851	110569.614657	35.965172
1407.020784	110728.198811	35.970189
1408.450039	110867.803438	35.975207
1409.716731	111030.070246	35.980224
1411.091073	111189.105427	35.985242
1413.048189	111353.676338	35.990260
1413.898456	111509.391361	35.995277
1415.518616	111660.376765	36.000295
1416.714312	111821.273783	36.005312
1417.903479	111993.940542	36.010330
1419.446111	112144.124635	36.015348
1420.918302	112313.697517	36.020365
1422.569804	112485.496625	36.025383
1424.221884	112633.526671	36.030400
1425.621048	112794.859778	36.035418
1426.999020	112957.963466	36.040436
1428.780848	113116.465156	36.045453
1430.121012	113271.841172	36.050471
1431.708201	113421.671396	36.055488
1433.186262	113583.813699	36.060506
1435.233611	113730.559333	36.065524
1436.402806	113884.807838	36.070541
1437.869324	114027.342714	36.075559
1439.157054	114180.510658	36.080576
1440.586594	114335.739800	36.085594
1441.892285	114482.189862	36.090612
1443.047408	114630.589256	36.095629
1444.947178	114777.453097	36.100647
1446.095798	114922.113735	36.105664
1446.922203	115062.287163	36.110682
1448.637655	115186.682749	36.115700
1449.795187	115350.121904	36.120717
1451.197999	115479.722005	36.125735
1452.836029	115634.121974	36.130752
1454.098680	115775.945742	36.135770
1455.363428	115939.403316	36.140788
1456.345092	116094.214273	36.145805
1458.040251	116250.793159	36.150823
1459.554884	116413.789888	36.155840
1460.774534	116561.367282	36.160858
1462.456335	116729.600739	36.165876
1463.717768	116900.073747	36.170893
1464.980844	117066.837444	36.175911
1466.425805	117228.292927	36.180928
1467.692033	117405.201256	36.185946
1469.544989	117573.356086	36.190964
1470.884707	117753.022002	36.195981
1472.403934	117922.935334	36.200999
1474.260171	118101.723838	36.206016
1475.349152	118270.840394	36.211034
1477.073867	118432.626233	36.216052
1478.585653	118621.990050	36.221069
1480.070501	118790.825503	36.226087
1482.195393	118963.828024	36.231104
1483.722822	119133.925318	36.236122
1485.806793	119284.091060	36.241140
1487.015030	119464.239339	36.246157
1488.548883	119617.875687	36.251175
1490.378067	119773.542929	36.256192
1491.453139	119952.797603	36.261210
1492.926986	120111.258780	36.266228
1494.605069	120278.350865	36.271245
1496.045725	120443.759384	36.276263
1497.329297	120612.841278	36.281280
1498.701515	120777.832190	36.286298
1500.467492	120951.373538	36.291316
1501.752553	121121.370330	36.296333
1503.456377	121288.705404	36.301351
1504.744435	121454.828445	36.306368
1506.288960	121620.531839	36.311386
1507.775104	121799.695834	36.316404
1509.048249	121961.822284	36.321421
1510.667905	122150.187663	36.326439
1511.969655	122325.445636	36.331456
1513.525774	122498.523905	36.336474
1515.268387	122668.103337	36.341492
1516.538970	122857.795753	36.346509
1517.843998	123031.284690	36.351527
1519.747183	123206.326272	36.356544
1521.181568	123401.531462	36.361562
1522.662995	123574.476614	36.366580
1524.407440	123752.637483	36.371597
1526.443086	123915.034693	36.376615
1527.931498	124073.770651	36.381632
1529.278528	124220.395786	36.386650
1530.683618	124377.056856	36.391668
1532.110489	124529.890142	36.396685
1533.656062	124684.605403	36.401703
1534.771348	124844.456511	36.406720
1536.121348	125009.021245	36.411738
1537.661683	125176.090077	36.416756
1539.139188	125356.520664	36.421773
1540.480699	125516.035810	36.426791
1541.885628	125691.122098	36.431808
1543.119980	125875.977522	36.436826
1544.841166	126045.163712	36.441844
1545.911007	126240.536079	36.446861
1547.814084	126417.637999	36.451879
1549.721292	126608.991149	36.456896
1551.299494	126788.414542	36.461914
1552.812363	126978.160830	36.466932
1554.463701	127165.922965	36.471949
1556.043031	127345.590522	36.476967
1557.956131	127531.312092	36.481984
1559.293038	127722.307595	36.487002
1561.208026	127905.244473	36.492020
1562.640767	128083.217311	36.497037
1564.133294	128264.298150	36.502055
1565.979164	128449.719905	36.507072
1567.442018	128642.944054	36.512090
1568.921301	128820.610219	36.517108
1570.690941	129013.078794	36.522125
1572.239336	129193.409411	36.527143
1573.917803	129380.168853	36.532160
1575.500499	129561.940636	36.537178
1577.346563	129734.917661	36.542196
1579.021876	129932.145706	36.547213
1580.618336	130105.570085	36.552231
1582.636464	130285.972528	36.557248
1583.678304	130469.698488	36.562266
1585.416147	130644.902767	36.567284
1586.990950	130819.006478	36.572301
1588.575072	130997.632738	36.577319
1590.397753	131177.793248	36.582336
1591.848628	131373.483422	36.587354
1593.491259	131550.418857	36.592372
1594.847610	131736.130269	36.597389
1596.525929	131932.890457	36.602407
1598.345210	132097.283555	36.607424
1599.859367	132289.688543	36.612442
1601.642732	132468.862617	36.617460
1603.267499	132654.448729	36.622477
1604.639537	132837.035360	36.627495
1606.837342	133011.991225	36.632512
1608.148738	133179.170019	36.637530
1610.045560	133352.921426	36.642548
1611.622536	133539.103731	36.647565
1613.145035	133706.087364	36.652583
1615.180810	133866.756509	36.657600
1616.318275	134028.899656	36.662618
1617.687621	134184.139344	36.667636
1619.461625	134324.516094	36.672653
1620.780084	134483.680763	36.677671
1622.372314	134646.958900	36.682688
1623.765494	134820.799196	36.687706
1625.464912	134982.465660	36.692724
1627.210741	135148.940701	36.697741
1628.722273	135319.179260	36.702759
1630.372711	135494.338571	36.707776
1631.587995	135667.261860	36.712794
1633.412689	135831.675534	36.717812
1635.243718	136008.874717	36.722829
1636.734098	136187.104797	36.727847
1638.145292	136368.034944	36.732864
1639.641089	136553.007744	36.737882
1641.328716	136727.281545	36.742900
1643.042374	136912.424768	36.747917
1644.535291	137108.679561	36.752935
1646.388400	137293.638307	36.757952
1647.810697	137480.884271	36.762970
1649.682479	137681.695394	36.767988
1651.156804	137871.482703	36.773005
1652.745519	138059.301511	36.778023
1654.634267	138251.902090	36.783040
1656.130633	138446.251693	36.788058
1658.064672	138628.037806	36.793076
1660.269654	138832.022685	36.798093
1661.951368	139032.442289	36.803111
1663.395258	139205.869670	36.808128
1665.127909	139399.947200	36.813146
1666.915955	139582.142522	36.818164
1668.613291	139764.619497	36.823181
1670.248167	139961.060733	36.828199
1672.245995	140139.652283	36.833216
1673.817054	140354.634617	36.838234
1675.448212	140529.497371	36.843252
1677.276329	140710.806046	36.848269
1678.910072	140901.068915	36.853287
1681.119966	141077.059609	36.858304
1682.675225	141257.793893	36.863322
1684.121170	141449.585545	36.868340
1686.174306	141627.289960	36.873357
1687.821261	141811.992603	36.878375
1689.475949	141997.430238	36.883392
1690.841476	142183.282473	36.888410
1692.405635	142374.934450	36.893428
1694.719529	142553.908320	36.898445
1696.063682	142746.155234	36.903463
1697.563456	142936.109911	36.908480
1699.513269	143111.114376	36.913498
1700.882241	143304.336789	36.918516
1702.763754	143484.791646	36.923533
1704.411801	143677.490448	36.928551
1705.884197	143832.079714	36.933568
1707.773205	144000.051681	36.938586
1709.296030	144177.031248	36.943604
1711.038668	144340.807540	36.948621
1712.544918	144522.468810	36.953639
1714.037133	144688.783706	36.958656
1715.921658	144866.837870	36.963674
1717.294465	145047.078416	36.968692
1719.112520	145232.763110	36.973709
1720.552138	145419.269530	36.978727
1722.492352	145594.454349	36.983744
1723.849542	145787.288483	36.988762
1725.397525	145977.380905	36.993780
1727.382932	146165.567032	36.998797
1728.905364	146355.310876	37.003815
1731.006962	146543.924474	37.008832
1732.675513	146765.134650	37.013850
1734.458846	146962.775922	37.018868
1735.900822	147157.164146	37.023885
1738.063280	147359.957616	37.028903
1739.857189	147555.357208	37.033920
1741.562580	147762.548460	37.038938
1743.483498	147949.449777	37.043956
1745.503082	148138.466191	37.048973
1747.231091	148350.018416	37.053991
1748.941124	148542.255536	37.059008
1750.880562	148738.539322	37.064026
1752.493307	148929.792746	37.069044
1754.225377	149131.613633	37.074061
1755.973170	149340.088744	37.079079
1757.906127	149520.265802	37.084096
1759.514201	149729.298052	37.089114
1760.947626	149942.682338	37.094132
1763.239200	150148.680322	37.099149
1764.801404	150347.797467	37.104167
1767.072801	150540.363050	37.109184
1768.879504	150738.137982	37.114202
1770.646830	150939.077108	37.119220
1772.430091	151140.141719	37.124237
1773.865084	151334.606998	37.129255
1776.135436	151534.595151	37.134272
1777.798041	151736.544678	37.139290
1779.426846	151932.580158	37.144308
1781.516045	152120.759335	37.149325
1783.172253	152336.241130	37.154343
1784.845269	152527.531476	37.159360
1786.644472	152727.119902	37.164378
1788.622782	152915.105681	37.169396
1790.383182	153110.189051	37.174413
1792.150598	153318.293364	37.179431
1794.598285	153504.242779	37.184448
1796.226783	153689.892210	37.189466
1797.898122	153892.069034	37.194484
1799.744500	154073.907724	37.199501
1801.415690	154261.468061	37.204519
1803.286285	154430.308921	37.209536
1805.290562	154594.260644	37.214554
1807.043660	154761.613014	37.219572
1808.712461	154921.866569	37.224589
1810.336676	155103.099461	37.229607
1812.018474	155276.665869	37.234624
1813.612515	155450.855710	37.239642
1815.405529	155628.134007	37.244660
1816.957111	155820.730392	37.249677
1818.475681	155999.360187	37.254695
1820.025115	156190.297978	37.259712
1822.045719	156397.037080	37.264730
1823.795333	156586.804134	37.269748
1825.645611	156786.307096	37.274765
1827.346022	156994.761706	37.279783
1829.232219	157184.053908	37.284800
1831.485986	157381.467473	37.289818
1833.146058	157592.734417	37.294836
1834.771551	157796.133700	37.299853
1836.546663	157997.887346	37.304871
1838.555838	158203.700784	37.309888
1840.246107	158421.574490	37.314906
1842.242953	158621.293047	37.319924
1843.914663	158833.174371	37.324941
1845.524583	159057.278323	37.329959
1847.816606	159266.172604	37.334976
1849.427042	159482.112763	37.339994
1851.248815	159703.004319	37.345012
1853.519091	159908.951221	37.350029
1855.322400	160135.529526	37.355047
1857.138418	160351.594562	37.360064
1859.358348	160557.515203	37.365082
1861.409004	160771.909681	37.370100
1863.309200	160981.180684	37.375117
1865.182268	161204.242005	37.380135
1867.189269	161405.965751	37.385152
1869.370099	161611.708488	37.390170
1871.054981	161827.194595	37.395188
1873.072645	162035.286423	37.400205
1875.038590	162251.529421	37.405223
1876.922059	162456.614028	37.410240
1878.664406	162666.642821	37.415258
1880.352742	162874.601548	37.420276
1882.752464	163079.214609	37.425293
1884.091304	163290.122729	37.430311
1886.165057	163488.791151	37.435328
1888.744708	163697.044327	37.440346
1890.121658	163909.383098	37.445364
1892.177637	164100.930154	37.450381
1894.269855	164316.594726	37.455399
1896.516070	164512.907764	37.460416
1897.894619	164719.848177	37.465434
1899.651448	164921.440991	37.470452
1901.853257	165122.368189	37.475469
1903.517317	165323.432563	37.480487
1905.225961	165510.463564	37.485504
1907.246031	165686.513289	37.490522
1908.708962	165877.732501	37.495540
1910.359802	166068.491645	37.500557
1912.371324	166264.458071	37.505575
1914.590851	166445.717923	37.510592
1916.059682	166639.324571	37.515610
1918.240993	166841.887807	37.520628
1920.134613	167028.846346	37.525645
1922.054072	167225.834422	37.530663
1923.257950	167431.029262	37.535680
1925.276990	167630.223288	37.540698
1927.403012	167847.754817	37.545716
1929.385523	168043.925399	37.550733
1931.067411	168258.346128	37.555751
1933.359287	168471.060394	37.560768
1935.644137	168679.553174	37.565786
1937.485312	168880.430926	37.570804
1939.667432	169089.170564	37.575821
1941.401150	169301.787783	37.580839
1943.187394	169504.529432	37.585856
1945.302391	169709.985178	37.590874
1947.131330	169928.996379	37.595892
1949.380279	170138.137017	37.600909
1951.026256	170360.097143	37.605927
1953.569787	170559.743278	37.610944
1955.372977	170773.156718	37.615962
1957.113571	170986.264141	37.620980
1959.081916	171199.628339	37.625997
1961.304461	171418.610855	37.631015
1962.950720	171631.051779	37.636032
1965.045137	171847.037988	37.641050
1966.805779	172077.260368	37.646068
1969.078902	172290.125471	37.651085
1971.330971	172506.952880	37.656103
1973.380449	172728.393048	37.661120
1975.672999	172940.624304	37.666138
1977.345007	173161.632058	37.671156
1979.440751	173359.168898	37.676173
1981.272495	173572.199725	37.681191
1983.285311	173798.408784	37.686208
1985.694429	174010.398897	37.691226
1987.551997	174222.401537	37.696244
1989.668783	174436.228991	37.701261
1991.866492	174639.515373	37.706279
1993.896157	174855.388631	37.711296
1996.015340	175052.676365	37.716314
1998.053208	175277.380107	37.721332
2000.128270	175475.032109	37.726349
2002.269597	175686.223533	37.731367
2004.066555	175898.942312	37.736384
2006.591812	176085.552127	37.741402
2008.487641	176293.575976	37.746420
2010.834298	176480.177869	37.751437
2012.616232	176671.031424	37.756455
2014.774465	176858.794042	37.761472
2016.862894	177010.462178	37.766490
2018.539768	177181.987528	37.771508
2020.286362	177358.082470	37.776525
2022.285826	177534.505956	37.781543
2024.137937	177700.816715	37.786560
2026.168388	177870.842502	37.791578
2028.177020	178053.432606	37.796596
2029.865373	178239.537901	37.801613
2031.953334	178436.478881	37.806631
2033.924784	178622.008097	37.811648
2035.821371	178797.755446	37.816666
2037.481479	179002.531565	37.821684
2039.720260	179210.198399	37.826701
2041.916462	179399.641155	37.831719
2043.793828	179586.635908	37.836736
2045.649116	179774.751493	37.841754
2047.978382	179988.726185	37.846772
2050.017468	180181.102817	37.851789
2052.563271	180372.803600	37.856807
2054.177724	180600.394509	37.861824
2056.371541	180796.314628	37.866842
2058.447193	181007.581386	37.871860
2061.063916	181200.416528	37.876877
2063.208422	181397.133858	37.881895
2064.775861	181613.356411	37.886912
2067.126225	181815.194346	37.891930
2069.364036	182010.795788	37.896948
2071.285813	182217.664675	37.901965
2073.617855	182417.554316	37.906983
2075.470760	182614.919766	37.912000
2078.132490	182809.201381	37.917018
2080.059395	183022.201770	37.922036
2082.576965	183214.604774	37.927053
2084.606064	183406.756207	37.932071
2086.645929	183604.439025	37.937088
2088.955727	183796.103514	37.942106
2090.925025	183994.941252	37.947124
2093.321397	184183.218463	37.952141
2095.308913	184379.466506	37.957159
2097.333254	184566.675043	37.962176
2099.586753	184751.754326	37.967194
2101.432416	184961.909182	37.972212
2103.561989	185159.229361	37.977229
2105.648193	185347.573358	37.982247
2107.524695	185545.392180	37.987264
2110.110305	185742.642565	37.992282
2112.029056	185938.210399	37.997300
2114.286974	186134.423188	38.002317
2116.535226	186332.884384	38.007335
2118.154335	186535.989081	38.012352
2120.497425	186723.536659	38.017370
2122.485828	186929.046287	38.022388
2124.762024	187123.382355	38.027405
2126.870584	187304.535855	38.032423
2128.777148	187473.476500	38.037440
2131.013465	187653.024883	38.042458
2132.904167	187819.926252	38.047476
2134.915770	187998.674089	38.052493
2136.902368	188168.632452	38.057511
2138.732097	188358.273104	38.062528
2140.953803	188529.692908	38.067546
2142.847460	188730.339878	38.072564
2145.116640	188911.550297	38.077581
2147.346804	189096.485829	38.082599
2149.344839	189301.737907	38.087616
2151.274456	189489.209937	38.092634
2153.419731	189688.285546	38.097652
2155.233767	189895.206434	38.102669
2157.347660	190089.593253	38.107687
2159.676121	190302.868375	38.112704
2162.038296	190501.887600	38.117722
2164.265889	190714.216071	38.122740
2166.364823	190917.783943	38.127757
2168.255599	191135.205890	38.132775
2170.521282	191348.559063	38.137792
2172.792578	191561.569634	38.142810
2175.047513	191776.373150	38.147828
2177.263318	191996.932821	38.152845
2179.511372	192199.847877	38.157863
2181.531234	192436.355129	38.162880
2183.913724	192647.576055	38.167898
2186.346588	192866.671118	38.172916
2188.506158	193078.627264	38.177933
2191.072444	193300.114424	38.182951
2193.063996	193504.382739	38.187968
2195.350857	193724.951570	38.192986
2197.677773	193934.752676	38.198004
2199.685445	194155.888040	38.203021
2202.121541	194364.302949	38.208039
2203.920521	194601.947016	38.213056
2206.430548	194809.412866	38.218074
2209.072629	195026.923160	38.223092
2211.224724	195250.159937	38.228109
2213.663745	195463.198726	38.233127
2215.627965	195676.999068	38.238144
2217.972930	195879.329873	38.243162
2220.139337	196107.289531	38.248180
2222.432794	196317.346963	38.253197
2225.026968	196539.364284	38.258215
2227.067771	196755.213087	38.263232
2229.136520	196960.561909	38.268250
2231.571935	197178.329878	38.273268
2233.746982	197395.416587	38.278285
2235.952509	197607.523961	38.283303
2237.828537	197824.545639	38.288320
2240.059859	198043.187275	38.293338
2242.181456	198259.181792	38.298356
2244.485049	198489.389389	38.303373
2246.868742	198700.546356	38.308391
2248.543964	198909.074895	38.313408
2250.920505	199093.148412	38.318426
2253.190674	199283.826972	38.323444
2255.057972	199495.754387	38.328461
2257.305036	199694.739171	38.333479
2259.384231	199908.068902	38.338496
2261.732225	200113.246057	38.343514
2263.766669	200330.887464	38.348532
2265.964328	200543.223554	38.353549
2268.315471	200757.528951	38.358567
2270.391553	200983.328029	38.363584
2272.753617	201195.551735	38.368602
2274.823801	201423.536791	38.373620
2276.928750	201653.776687	38.378637
2279.660405	201861.844420	38.383655
2281.656252	202104.720687	38.388672
2284.183689	202335.480320	38.393690
2286.693068	202564.365132	38.398708
2288.638658	202788.757899	38.403725
2291.238196	203019.001178	38.408743
2293.194517	203262.167995	38.413760
2295.793453	203499.699500	38.418778
2298.112291	203738.825054	38.423796
2300.594662	203980.972204	38.428813
2302.942867	204215.030263	38.433831
2305.254702	204451.240320	38.438848
2307.805028	204690.434704	38.443866
2310.161433	204913.514012	38.448884
2312.746953	205148.185637	38.453901
2315.262873	205374.859246	38.458919
2317.639766	205603.282192	38.463936
2319.621290	205840.692765	38.468954
2321.946593	206070.674412	38.473972
2324.261887	206313.390967	38.478989
2326.726335	206542.908095	38.484007
2328.972200	206796.123206	38.489024
2331.534066	207022.910138	38.494042
2333.593676	207265.239513	38.499060
2336.029334	207505.580670	38.504077
2338.827904	207745.776391	38.509095
2340.727828	207988.159389	38.514112
2343.142310	208226.475628	38.519130
2345.631415	208466.596329	38.524148
2347.684494	208709.808477	38.529165
2350.125993	208948.567578	38.534183
2352.410574	209205.518953	38.539200
2354.499332	209448.499861	38.544218
2356.834903	209697.574302	38.549236
2358.976175	209952.824974	38.554253
2361.933166	210203.339032	38.559271
2364.145881	210463.417316	38.564288
2366.596705	210700.378961	38.569306
2369.191278	210949.252289	38.574324
2370.960971	211202.434135	38.579341
2373.625550	211436.482806	38.584359
2376.093539	211672.670946	38.589376
2377.968044	211890.761406	38.594394
2380.201682	212112.071122	38.599412
2382.468983	212347.341393	38.604429
2385.020838	212562.190942	38.609447
2386.826740	212791.429377	38.614464
2389.296291	213039.987850	38.619482
2391.602794	213274.772825	38.624500
2393.330313	213516.188760	38.629517
2395.981748	213756.494233	38.634535
2398.290913	214024.252582	38.639552
2400.348837	214282.009340	38.644570
2402.717781	214527.351889	38.649588
2405.261747	214802.820698	38.654605
2407.834098	215059.076939	38.659623
2410.275432	215329.777741	38.664640
2412.569388	215593.507378	38.669658
2415.484213	215870.432588	38.674676
2417.567069	216136.406927	38.679693
2420.291975	216407.854216	38.684711
2422.843918	216678.631686	38.689728
2425.076482	216947.073903	38.694746
2427.498686	217231.027600	38.699764
2430.051460	217501.389144	38.704781
2432.808133	217763.187297	38.709799
2435.284784	218046.031043	38.714816
2437.704008	218319.184745	38.719834
2440.137432	218588.375858	38.724852
2442.487300	218872.474551	38.729869
2444.981707	219137.442717	38.734887
2447.631026	219416.899830	38.739904
2450.437568	219695.495097	38.744922
2452.995826	219963.858924	38.749940
2455.164058	220242.532043	38.754957
2458.267451	220510.582910	38.759975
2460.665245	220788.764601	38.764992
2463.051645	221063.673266	38.770010
2465.709801	221332.178563	38.775028
2468.347906	221604.294014	38.780045
2471.018307	221878.767019	38.785063
2473.131585	222145.622023	38.790080
2475.531342	222411.886564	38.795098
2478.107167	222688.739173	38.800116
2480.574585	222960.048457	38.805133
2483.173558	223225.090658	38.810151
2485.355120	223516.826700	38.815168
2487.997541	223844.221873	38.820186
2490.795405	224113.565431	38.825204
2492.892284	224391.401480	38.830221
2495.364869	224667.807593	38.835239
2497.625048	224945.683167	38.840256
2500.232527	225234.589865	38.845274
2502.939114	225504.587436	38.850292
2505.260978	225785.402008	38.855309
2507.827417	226047.398489	38.860327
2510.451453	226308.408927	38.865344
2512.588228	226560.024664	38.870362
2514.709356	226800.418537	38.875380
2517.203989	227059.674096	38.880397
2519.240824	227323.574335	38.885415
2521.965287	227582.083975	38.890432
2524.044926	227843.718763	38.895450
2526.700492	228119.307368	38.900468
2528.819219	228401.178700	38.905485
2531.466279	228669.811729	38.910503
2533.798956	228953.149346	38.915520
2536.060662	229234.746738	38.920538
2538.597957	229531.209363	38.925556
2541.199800	229828.043702	38.930573
2543.597698	230122.803379	38.935591
2545.970740	230422.799781	38.940608
2548.818088	230732.169804	38.945626
2551.683380	231030.693353	38.950644
2553.901813	231342.095288	38.955661
2556.965769	231641.605228	38.960679
2559.411457	231952.516038	38.965696
2561.804449	232270.852354	38.970714
2564.711136	232570.212387	38.975732
2567.355680	232881.272518	38.980749
2569.999542	233182.199981	38.985767
2572.561296	233493.249804	38.990784
2575.052656	233806.038843	38.995802
2578.236406	234107.924940	39.000820
2580.790061	234429.620848	39.005837
2583.682920	234726.830839	39.010855
2586.556814	235035.372408	39.015872
2588.962918	235339.620495	39.020890
2591.617627	235642.915750	39.025908
2594.143372	235941.051009	39.030925
2596.926824	236253.217183	39.035943
2599.183982	236563.410374	39.040960
2601.941863	236873.855328	39.045978
2604.974129	237180.600269	39.050996
2607.017623	237492.811142	39.056013
2609.851709	237804.948457	39.061031
2612.687497	238105.224991	39.066048
2615.171184	238416.454400	39.071066
2617.895039	238722.084188	39.076084
2620.610628	239034.700948	39.081101
2623.239580	239347.383102	39.086119
2625.926179	239653.453113	39.091136
2628.658507	239964.723609	39.096154
2631.160732	240260.842415	39.101172
2633.815705	240576.317748	39.106189
2636.803478	240886.585050	39.111207
2639.404534	241185.763901	39.116224
2641.849629	241504.983330	39.121242
2644.765955	241801.853178	39.126260
2647.393774	242106.999064	39.131277
2649.805312	242402.883537	39.136295
2652.290004	242685.549050	39.141312
2654.507186	242970.264196	39.146330
2657.457369	243236.905882	39.151348
2659.540328	243529.390624	39.156365
2662.269895	243814.661496	39.161383
2664.459774	244105.987589	39.166400
2666.848680	244408.509816	39.171418
2669.631218	244697.558893	39.176436
2672.097009	245004.439190	39.181453
2674.508988	245309.118853	39.186471
2677.053677	245622.312814	39.191488
2679.656911	245935.066400	39.196506
2682.542460	246258.596721	39.201524
2685.033894	246580.793169	39.206541
2687.748783	246904.758416	39.211559
2690.636400	247236.063322	39.216576
2692.946295	247561.465845	39.221594
2695.619907	247889.427788	39.226612
2698.299415	248234.814720	39.231629
2701.311483	248578.092265	39.236647
2704.201813	248916.385812	39.241664
2706.947557	249266.159003	39.246682
2709.954995	249593.614500	39.251700
2712.670240	249929.728044	39.256717
2715.236214	250276.890183	39.261735
2718.151551	250613.430676	39.266752
2720.770322	250959.595233	39.271770
2723.789784	251298.101941	39.276788
2726.502040	251652.330834	39.281805
2729.102935	251985.799454	39.286823
2732.082578	252339.885787	39.291840
2734.557613	252692.782654	39.296858
2737.895988	253035.382707	39.301876
2740.341413	253397.023881	39.306893
2743.410332	253735.756009	39.311911
2746.535030	254085.199570	39.316928
2748.994362	254437.289356	39.321946
2752.277064	254774.693945	39.326964
2754.563546	255125.389812	39.331981
2757.304344	255459.274268	39.336999
2760.274811	255804.477700	39.342016
2762.918541	256155.448966	39.347034
2765.790002	256498.154382	39.352052
2768.341959	256855.669722	39.357069
2771.270154	257207.105678	39.362087
2774.418731	257552.690115	39.367104
2777.013255	257904.179988	39.372122
2779.889133	258250.062672	39.377140
2782.603851	258590.484422	39.382157
2785.316121	258945.970778	39.387175
2788.204555	259294.393208	39.392192
2790.944909	259644.439932	39.397210
2793.701847	259989.480165	39.402228
2796.544203	260338.520948	39.407245
2798.884757	260680.503464	39.412263
2801.796485	261002.861190	39.417280
2804.207052	261329.058263	39.422298
2806.962575	261651.009599	39.427316
2809.459598	261984.712946	39.432333
2812.198327	262311.621204	39.437351
2814.690599	262639.534140	39.442368
2817.014727	262986.881897	39.447386
2819.915301	263324.256971	39.452404
2822.775256	263672.562105	39.457421
2825.530611	264039.199736	39.462439
2828.624346	264389.119745	39.467456
2831.111676	264751.304181	39.472474
2834.159757	265104.229637	39.477492
2836.914848	265463.501774	39.482509
2839.957002	265833.753732	39.487527
2842.808890	266198.091791	39.492544
2845.233211	266579.772017	39.497562
2848.347653	266937.235627	39.502580
2851.498615	267314.000170	39.507597
2854.188172	267686.087640	39.512615
2857.241037	268058.270260	39.517632
2859.933929	268444.278699	39.522650
2863.164322	268820.117169	39.527668
2865.826057	269204.047945	39.532685
2868.540906	269577.732987	39.537703
2871.882876	269951.445944	39.542720
2874.432501	270350.814903	39.547738
2877.533351	270733.076524	39.552756
2880.747948	271121.620332	39.557773
2883.407355	271504.002963	39.562791
2886.722023	271887.094890	39.567808
2889.412493	272268.329703	39.572826
2892.784700	272648.415145	39.577844
2895.582627	273045.561077	39.582861
2898.430424	273425.501088	39.587879
2901.632386	273807.671397	39.592896
2904.311492	274202.219791	39.597914
2907.401297	274585.398679	39.602932
2910.351147	274969.615885	39.607949
2913.137405	275355.586432	39.612967
2916.097113	275734.467363	39.617984
2919.054411	276133.391954	39.623002
2922.278103	276524.145242	39.628020
2924.824187	276914.142040	39.633037
2927.793264	277311.819849	39.638055
2930.714776	277695.202991	39.643072
2933.699120	278097.527029	39.648090
2936.514169	278483.263940	39.653108
2939.568126	278868.048388	39.658125
2942.410465	279273.417529	39.663143
2945.506442	279671.201557	39.668160
2948.279283	280079.299517	39.673178
2951.269278	280465.541440	39.678196
2954.184450	280867.494267	39.683213
2957.013053	281257.825860	39.688231
2960.234597	281621.319959	39.693248
2962.819050	281986.311882	39.698266
2965.556493	282350.847509	39.703284
2968.419654	282708.631145	39.708301
2971.016290	283082.994234	39.713319
2974.014828	283452.085777	39.718336
2976.848209	283830.830995	39.723354
2979.405518	284202.989385	39.728372
2982.319662	284586.166755	39.733389
2985.122175	284986.889610	39.738407
2988.337301	285378.096818	39.743424
2991.285836	285783.444545	39.748442
2994.154390	286187.839190	39.753460
2997.419904	286589.554053	39.758477
3000.145924	287001.362634	39.763495
3003.144997	287411.425506	39.768512
3005.717133	287829.633580	39.773530
3008.676050	288249.329468	39.778548
3011.844159	288674.427893	39.783565
3014.887763	289111.484749	39.788583
3018.361381	289534.755395	39.793600
3021.513176	289957.974738	39.798618
3024.402718	290395.562061	39.803636
3027.252365	290805.288274	39.808653
3029.988272	291245.108540	39.813671
3033.931130	291692.306987	39.818688
3037.031788	292127.749540	39.823706
3039.757290	292560.456410	39.828724
3042.790268	293000.836157	39.833741
3045.733939	293443.693223	39.838759
3049.416224	293881.936303	39.843776
3052.410839	294328.111238	39.848794
3055.071777	294770.095877	39.853812
3058.313881	295204.620974	39.858829
3061.601337	295657.732314	39.863847
3064.817138	296095.358712	39.868864
3068.043808	296552.389533	39.873882
3071.502956	296978.442915	39.878900
3074.606784	297437.446987	39.883917
3077.409391	297884.406318	39.888935
3080.464710	298316.769345	39.893952
3083.829432	298752.790995	39.898970
3087.326970	299189.069948	39.903988
3090.492791	299639.421933	39.909005
3093.325406	300077.835931	39.914023
3096.656458	300520.843741	39.919040
3099.697383	300961.914940	39.924058
3102.520621	301391.639587	39.929076
3105.890427	301826.483804	39.934093
3108.761027	302275.630415	39.939111
3111.914260	302706.340600	39.944128
3115.651275	303156.134896	39.949146
3118.347960	303592.426741	39.954164
3121.567268	304025.027647	39.959181
3125.028132	304447.530312	39.964199
3127.987680	304847.275820	39.969216
3130.467826	305252.506351	39.974234
3133.730326	305648.366089	39.979252
3137.035453	306038.121805	39.984269
3139.851113	306449.213931	39.989287
3142.920461	306846.904070	39.994304
3145.779150	307253.871990	39.999322
3148.703685	307671.623244	40.004340
3151.800958	308090.082378	40.009357
3154.634238	308506.981673	40.014375
3157.493566	308940.994936	40.019392
3160.595877	309374.739598	40.024410
3163.665372	309816.895168	40.029428
3166.718629	310259.915234	40.034445
3169.550041	310712.163325	40.039463
3173.027789	311151.836277	40.044480
3176.372593	311612.305172	40.049498
3179.214349	312069.295878	40.054516
3182.442962	312530.922317	40.059533
3185.591027	312994.820057	40.064551
3188.900972	313458.385405	40.069568
3191.823992	313936.436434	40.074586
3195.403932	314413.035235	40.079604
3198.645502	314882.649999	40.084621
3201.641322	315363.121208	40.089639
3205.036060	315852.035450	40.094656
3208.157458	316336.469684	40.099674
3211.698144	316831.172208	40.104692
3214.915957	317297.858650	40.109709
3218.577538	317781.082777	40.114727
3221.819207	318265.259811	40.119744
3224.654164	318759.225951	40.124762
3228.105961	319241.739282	40.129780
3231.856363	319720.317083	40.134797
3234.855034	320218.389287	40.139815
3238.628973	320698.024906	40.144832
3242.032173	321176.243588	40.149850
3245.351842	321664.352216	40.154868
3248.519683	322135.822013	40.159885
3251.948973	322618.244537	40.164903
3255.865681	323100.257101	40.169920
3258.674987	323585.895978	40.174938
3262.090856	324054.522393	40.179956
3265.676344	324519.411555	40.184973
3268.609743	325007.054199	40.189991
3271.911952	325477.442825	40.195008
3275.198193	325955.195909	40.200026
3278.459012	326440.187813	40.205044
3281.843481	326917.614865	40.210061
3285.160162	327394.237110	40.215079
3288.218827	327866.783304	40.220096
3291.556920	328348.906973	40.225114
3294.748721	328833.564801	40.230132
3298.385523	329309.413518	40.235149
3301.067553	329770.707042	40.240167
3304.412705	330219.398999	40.245184
3307.553188	330661.670578	40.250202
3310.419643	331107.715706	40.255220
3313.347553	331554.992666	40.260237
3316.142212	332013.257865	40.265255
3319.582287	332468.269302	40.270272
3322.724975	332942.953672	40.275290
3325.401490	333418.419577	40.280308
3329.073817	333892.658267	40.285325
3332.107174	334387.562697	40.290343
3335.022672	334882.685349	40.295360
3338.502135	335386.246971	40.300378
3341.514338	335878.985606	40.305396
3345.154115	336393.813760	40.310413
3348.565285	336904.484484	40.315431
3351.923177	337413.686986	40.320448
3355.152448	337936.896393	40.325466
3358.411226	338462.661403	40.330484
3362.144658	338975.854818	40.335501
3365.347227	339502.204184	40.340519
3368.634967	340041.687891	40.345536
3372.435935	340565.521678	40.350554
3376.015651	341097.256913	40.355572
3379.161622	341636.977740	40.360589
3382.875623	342174.242774	40.365607
3386.342129	342698.162086	40.370624
3390.001302	343235.832605	40.375642
3393.190331	343772.455534	40.380660
3397.083012	344301.777396	40.385677
3400.589828	344838.137303	40.390695
3403.868918	345375.772317	40.395712
3407.689168	345908.442318	40.400730
3410.868635	346455.831969	40.405748
3414.565021	346983.459447	40.410765
3418.075548	347518.702155	40.415783
3421.673316	348057.099341	40.420800
3425.211568	348595.906939	40.425818
3428.561079	349148.549335	40.430836
3432.021275	349663.165659	40.435853
3435.555041	350207.949327	40.440871
3438.761140	350739.324955	40.445888
3442.583523	351278.518143	40.450906
3446.112974	351812.675191	40.455924
3449.733096	352346.076375	40.460941
3453.289847	352886.970647	40.465959
3456.696217	353424.405460	40.470976
3460.108751	353949.497085	40.475994
3463.577232	354485.565730	40.481012
3467.172690	355016.202006	40.486029
3470.794914	355551.727507	40.491047
3473.926967	356092.858343	40.496064
3477.642986	356627.469203	40.501082
3480.761157	357161.585068	40.506100
3484.255882	357698.376937	40.511117
3487.769951	358219.459790	40.516122
3490.998333	358710.783865	40.521127
3494.186659	359144.346103	40.526132
3496.993383	359539.337539	40.531136
3499.614587	359870.485694	40.536141
3501.859292	360151.486481	40.541146
3504.139937	360409.629708	40.546151
3506.463368	360596.695273	40.551156
3507.799661	360762.414707	40.556160
3509.359252	360869.268414	40.561165
3510.596290	360957.063376	40.566170
3511.897717	361004.720651	40.571175
3513.217598	361033.265496	40.576180
3513.926432	361035.112961	40.581184
3514.596430	360994.243783	40.586189
3515.203160	360955.878222	40.591194
3515.536493	360895.850896	40.596199
3515.692954	360806.690938	40.601204
3516.039501	360718.442249	40.606208
3516.093115	360611.002842	40.611213
3516.231807	360506.501440	40.616218
3516.250951	360385.682564	40.621223
3516.884291	360261.585567	40.626228
3516.570831	360129.953278	40.631232
3516.507161	359979.425713	40.636237
3516.350389	359852.628066	40.641242
3515.894598	359705.138811	40.646247
3515.905319	359556.710189	40.651252
3515.292491	359414.384992	40.656256
3515.493440	359271.065557	40.661261
3514.970047	359145.265523	40.666266
3515.040972	358992.041735	40.671271
3514.690805	358852.955959	40.676276
3514.428172	358718.130975	40.681280
3514.116331	358567.027534	40.686285
3514.100200	358452.978219	40.691290
3513.502014	358306.779564	40.696295
3513.475497	358182.603433	40.701300
3512.881929	358057.167943	40.706304
3512.932295	357923.741766	40.711309
3512.609181	357809.281439	40.716314
3512.383461	357680.987663	40.721319
3512.339499	357555.489458	40.726324
3512.097959	357448.013375	40.731328
3511.737695	357329.918854	40.736333
3511.586944	357219.247009	40.741338
3511.304020	357123.380760	40.746343
3511.252666	357021.701145	40.751348
3510.837440	356910.561474	40.756352
3510.619092	356808.322529	40.761357
3510.317541	356717.344378	40.766362
3509.851075	356629.598537	40.771367
3510.192532	356526.328955	40.776372
3509.750544	356442.497865	40.781376
3509.555816	356354.937615	40.786381
3509.353937	356277.582928	40.791386
3509.298004	356191.043812	40.796391
3509.328908	356119.276064	40.801396
3508.678248	356058.304103	40.806400
3508.857998	355971.065703	40.811405
3508.572288	355901.510778	40.816410
3508.375473	355830.363923	40.821415
3508.638455	355758.940695	40.826420
3508.201351	355693.582906	40.831424
3508.279713	355626.234931	40.836429
3507.516527	355567.977671	40.841434
3507.695624	355510.742000	40.846439
3507.744171	355450.091388	40.851444
3507.567051	355398.306934	40.856448
3507.483069	355333.452718	40.861453
3507.327487	355286.881651	40.866458
3507.205434	355236.818814	40.871463
3507.442881	355189.574764	40.876468
3507.041001	355133.931969	40.881472
3506.882682	355091.509247	40.886477
3506.915562	355029.995364	40.891482
3506.861384	354984.324135	40.896487
3506.879320	354938.514221	40.901492
3506.356605	354902.587423	40.906496
3506.560257	354840.944521	40.911501
3506.469322	354816.274012	40.916506
3506.209850	354776.360980	40.921511
3506.536232	354743.226426	40.926516
3506.566268	354710.622223	40.931520
3506.368368	354664.464456	40.936525
3506.197205	354637.719755	40.941530
3506.159038	354591.129491	40.946535
3506.026517	354551.883329	40.951540
3505.915574	354525.358088	40.956544
3506.195256	354486.657481	40.961549
3506.183811	354453.194415	40.966554
3505.768823	354410.480872	40.971559
3506.036332	354374.454227	40.976564
3505.858332	354352.393036	40.981568
3505.699620	354318.138802	40.986573
3505.523119	354293.176182	40.991578
3505.697433	354262.737486	40.996583
3505.629595	354241.549542	41.001588
3505.261274	354225.269827	41.006592
3505.567728	354187.633615	41.011597
3505.588879	354165.337269	41.016602
3505.393581	354133.531791	41.021607
3505.418799	354110.751249	41.026612
3505.559504	354092.126065	41.031616
3505.597164	354063.108547	41.036621
3505.270048	354040.536368	41.041626
3505.461160	354011.138276	41.046631
3505.382448	353978.041821	41.051636
3505.410619	353957.093072	41.056640
3505.382085	353921.138361	41.061645
3505.441318	353908.633755	41.066650
3505.227916	353885.967185	41.071655
3505.318361	353858.340903	41.076660
3505.231092	353830.640906	41.081664
3505.403707	353817.914761	41.086669
3504.858841	353786.546068	41.091674
3505.064984	353767.172399	41.096679
3504.837531	353743.719065	41.101684
3504.825516	353728.782566	41.106688
3504.785312	353706.724764	41.111693
3504.864004	353689.967025	41.116698
3504.904989	353676.727224	41.121703
3505.005599	353653.883664	41.126708
3504.514011	353645.868776	41.131712
3504.922737	353619.795348	41.136717
3504.642268	353603.501548	41.141722
3504.487000	353593.677490	41.146727
3505.118973	353573.116666	41.151732
3504.500864	353562.525950	41.156736
3504.296863	353538.865223	41.161741
3504.379940	353529.970543	41.166746
3504.660523	353522.698838	41.171751
3504.706396	353502.052497	41.176756
3504.466547	353497.382536	41.181760
3504.910088	353478.480214	41.186765
3504.884345	353467.312296	41.191770
3504.845223	353445.508705	41.196775
3504.977000	353427.164636	41.201780
3504.738524	353406.537761	41.206784
3504.906914	353383.810614	41.211789
3504.616590	353378.665085	41.216794
3504.822611	353351.274755	41.221799
3504.564879	353340.270732	41.226804
3504.544840	353330.552493	41.231808
3504.899323	353310.340825	41.236813
3504.792425	353302.290518	41.241818
3504.623688	353280.074710	41.246823
3504.915255	353262.468802	41.251828
3504.899563	353255.625637	41.256832
3504.667196	353232.681837	41.261837
3504.727983	353213.407290	41.266842
3504.683549	353191.451736	41.271847
3504.593523	353174.236966	41.276852
3504.522684	353162.643473	41.281856
3504.653355	353139.667689	41.286861
3504.618108	353133.438385	41.291866
3504.278885	353117.230069	41.296871
3504.618450	353096.282644	41.301876
3504.411043	353091.658416	41.306880
3504.520274	353072.783350	41.311885
3504.401750	353053.333495	41.316890
3504.352156	353045.503134	41.321895
3504.488380	353024.206085	41.326900
3504.439974	353027.191551	41.331904
3504.431830	353005.128384	41.336909
3504.411182	352991.287365	41.341914
3504.132052	352974.229672	41.346919
3504.406188	352964.108566	41.351924
3504.142620	352957.533595	41.356928
3504.188351	352938.363124	41.361933
3504.289866	352940.637758	41.366938
3504.275004	352925.599680	41.371943
3504.422630	352910.994002	41.376948
3504.315349	352906.048534	41.381952
3504.392034	352893.591825	41.386957
3504.209334	352878.656616	41.391962
3503.904521	352874.022318	41.396967
3504.189093	352861.965379	41.401972
3504.178888	352853.747019	41.406976
3504.331813	352847.513383	41.411981
3504.514143	352833.309389	41.416986
3504.241523	352825.310657	41.421991
3504.394093	352817.092008	41.426996
3503.923154	352804.289209	41.432000
3504.180086	352800.049640	41.437005
3504.309719	352786.846498	41.442010
3504.210588	352777.751450	41.447015
3504.617182	352759.949042	41.452020
3504.448000	352751.654000	41.457024
3504.505247	352719.451439	41.462029
3504.881149	352719.137744	41.467034
3504.562408	352694.604038	41.472039
3504.555629	352684.349141	41.477044
3503.960053	352662.964038	41.482048
3504.374204	352645.694839	41.487053
3504.395170	352632.508837	41.492058
3503.841792	352638.017322	41.497063
3504.599142	352621.126503	41.502068
3504.376943	352590.978563	41.507072
3504.414494	352589.878518	41.512077
3504.149573	352584.092653	41.517082
3504.225842	352571.635933	41.522087
3504.367770	352548.632661	41.527092
3504.055563	352552.677846	41.532096
3504.528980	352533.286917	41.537101
3504.386241	352522.773536	41.542106
3504.253579	352512.131311	41.547111
3504.307789	352489.574526	41.552116
3503.977733	352487.234659	41.557120
3504.524554	352468.900990	41.562125
3504.156869	352479.419180	41.567130
3504.007605	352456.716400	41.572135
3504.397875	352436.524189	41.577140
3503.933817	352446.726775	41.582144
3504.098906	352415.754016	41.587149
3504.146334	352408.519016	41.592154
3503.883311	352411.843843	41.597159
3504.285127	352390.555450	41.602164
3503.885671	352391.814966	41.607168
3503.923212	352389.467880	41.612173
3503.887339	352373.465876	41.617178
3504.165783	352366.906942	41.622183
3504.533336	352352.749886	41.627188
3504.248196	352347.323489	41.632192
3504.344373	352324.887247	41.637197
3504.353150	352305.569690	41.642202
3504.132597	352299.420482	41.647207
3504.018938	352282.692702	41.652212
3504.163556	352281.473926	41.657216
3503.991889	352271.270465	41.662221
3503.856129	352257.752849	41.667226
3504.158228	352250.044919	41.672231
3504.399890	352245.604122	41.677236
3503.943473	352236.031017	41.682240
3504.143181	352223.249303	41.687245
3504.270135	352206.534360	41.692250
3504.142845	352202.889932	41.697255
3504.228965	352183.076556	41.702260
3504.144061	352173.241108	41.707264
3504.529600	352167.785013	41.712269
3504.307410	352150.870751	41.717274
3504.269225	352137.108629	41.722279
3504.278683	352112.344618	41.727284
3503.941004	352112.092830	41.732288
3504.083643	352107.565876	41.737293
3504.187445	352094.392094	41.742298
3504.065508	352089.576116	41.747303
3504.165293	352076.810164	41.752308
3503.786693	352059.716999	41.757312
3503.897242	352057.765556	41.762317
3504.071294	352055.473225	41.767322
3504.216086	352047.052087	41.772327
3504.168813	352032.553327	41.777332
3504.234462	352027.987637	41.782336
3504.155716	352010.083555	41.787341
3504.035711	352002.340520	41.792346
3503.729910	351978.389784	41.797351
3503.699171	351976.053474	41.802356
3503.791003	351985.430219	41.807360
3504.198980	351973.099069	41.812365
3504.096234	351961.281305	41.817370
3503.897218	351954.670553	41.822375
3504.049749	351947.138924	41.827380
3503.766748	351934.687952	41.832384
3503.888400	351933.574598	41.837389
3504.042246	351929.096757	41.842394
3504.071854	351910.386562	41.847399
3504.238871	351909.291486	41.852404
3503.558926	351903.469357	41.857408
3504.194910	351873.032637	41.862413
3504.078720	351879.693686	41.867418
3503.969776	351868.436781	41.872423
3504.236391	351848.263895	41.877428
3503.847674	351847.129424	41.882432
3503.930742	351842.662765	41.887437
3504.192119	351820.963695	41.892442
3504.131856	351821.100700	41.897447
3503.928228	351811.385754	41.902452
3503.944073	351799.651006	41.907456
3503.953795	351792.778184	41.912461
3503.899152	351794.492203	41.917466
3503.746641	351774.818200	41.922471
3503.816222	351761.140744	41.927476
3503.850158	351766.149269	41.932480
3503.406425	351758.177426	41.937485
3504.013251	351750.472150	41.942490
3504.064041	351740.666071	41.947495
3503.901013	351740.081270	41.952500
3503.644591	351727.727847	41.957504
3504.101071	351713.811064	41.962509
3504.070381	351714.554196	41.967514
3503.712347	351706.670597	41.972519
3503.600120	351687.142893	41.977524
3503.799624	351686.653479	41.982528
3503.640430	351685.304568	41.987533
3503.712899	351693.742772	41.992538
3503.660529	351688.228607	41.997543
3503.775822	351677.826967	42.002548
3503.689252	351671.147502	42.007552
3503.695387	351682.955609	42.012557
3503.892146	351679.056315	42.017562
3503.669469	351666.035840	42.022567
3503.718069	351657.655298	42.027572
3503.812655	351657.182470	42.032576
3503.883000	351655.593670	42.037581
3504.154361	351643.996644	42.042586
3503.888261	351634.953246	42.047591
3504.332631	351636.232079	42.052596
3503.885798	351619.709463	42.057600
3504.268392	351619.343805	42.062605
3503.993980	351598.925503	42.067610
3503.795681	351589.336925	42.072615
3503.864505	351579.960618	42.077620
3503.767422	351588.578344	42.082624
3503.834162	351567.851596	42.087629
3503.777750	351561.523652	42.092634
3503.917091	351548.115065	42.097639
3504.186400	351545.934904	42.102644
3503.531247	351544.180842	42.107648
3503.668632	351520.490689	42.112653
3503.940869	351518.920868	42.117658
3503.660155	351523.190203	42.122663
3503.821195	351504.026434	42.127668
3503.987227	351497.485165	42.132672
3504.057773	351486.759709	42.137677
3503.869288	351485.008220	42.142682
3503.648689	351472.623625	42.147687
3504.055676	351469.989041	42.152692
3503.670258	351468.904940	42.157696
3503.705494	351447.343270	42.162701
3503.940537	351449.775010	42.167706
3503.748648	351446.242544	42.172711
3504.174181	351430.014610	42.177716
3504.135919	351427.094110	42.182720
3503.905942	351415.041837	42.187725
3503.848612	351417.672502	42.192730
3503.548046	351395.883945	42.197735
3504.134808	351378.841549	42.202740
3503.814221	351386.756584	42.207744
3504.244164	351382.769504	42.212749
3504.280322	351357.288314	42.217754
3503.816110	351360.161457	42.222759
3504.053985	351327.395040	42.227764
3503.609953	351328.076271	42.232768
3503.695551	351326.714102	42.237773
3503.645628	351330.107108	42.242778
3503.499874	351317.227089	42.247783
3503.523628	351294.140155	42.252788
3503.516081	351304.601643	42.257792
3503.588118	351295.402930	42.262797
3503.894361	351305.382155	42.267802
3503.669602	351301.193168	42.272807
3503.906231	351282.297323	42.277812
3503.633836	351276.487046	42.282816
3504.052884	351270.083902	42.287821
3503.847387	351266.986230	42.292826
3503.709709	351251.330836	42.297831
3503.844784	351241.231386	42.302836
3503.745217	351250.460367	42.307840
3503.826692	351247.775431	42.312845
3503.899605	351230.941475	42.317850
3503.577304	351230.101894	42.322855
3503.967435	351227.775367	42.327860
3503.847255	351221.559266	42.332864
3503.974008	351201.993604	42.337869
3503.983865	351209.423769	42.342874
3503.761285	351214.549250	42.347879
3504.130812	351177.842578	42.352884
3503.931963	351174.133041	42.357888
3503.992696	351170.077063	42.362893
3503.825859	351156.971285	42.367898
3503.812204	351146.411774	42.372903
3503.980166	351140.099210	42.377908
3503.669026	351129.917580	42.382912
3503.892022	351121.585734	42.387917
3503.654487	351112.155975	42.392922
3503.410591	351114.256241	42.397927
3503.774618	351121.834030	42.402932
3503.688155	351116.885105	42.407936
3503.585234	351095.243332	42.412941
3503.454116	351103.077555	42.417946
3503.688424	351094.005856	42.422951
3503.891486	351094.432088	42.427956
3503.790428	351087.627589	42.432960
3503.964294	351071.108478	42.437965
3503.553248	351064.073028	42.442970
3503.822307	351070.469669	42.447975
3503.884236	351055.138967	42.452980
3503.740614	351051.013485	42.457984
3503.938435	351041.718491	42.462989
3503.809198	351041.026539	42.467994
3503.751764	351021.108173	42.472999
3503.663228	351006.055748	42.478004
3503.433878	351021.438838	42.483008
3503.796660	351005.042543	42.488013
3503.840821	351004.017772	42.493018
3503.597572	350995.047004	42.498023
3503.938318	350979.239544	42.503028
3503.709616	350986.071194	42.508032
3503.940532	350978.985145	42.513037
3503.887243	350956.571958	42.518042
3503.658089	350952.103683	42.523047
3504.117863	350950.224243	42.528052
3503.572777	350939.392398	42.533056
3503.910487	350918.724364	42.538061
3503.836162	350919.983415	42.543066
3503.636460	350925.767018	42.548071
3503.878122	350915.014396	42.553076
3503.648495	350897.388298	42.558080
3503.702283	350887.454336	42.563085
3503.573964	350892.310440	42.568090
3503.453596	350895.841863	42.573095
3503.609774	350890.981809	42.578100
3503.503429	350877.051985	42.583104
3503.561602	350874.981527	42.588109
3503.678101	350877.890143	42.593114
3503.553054	350878.419149	42.598119
3504.004692	350866.157193	42.603124
3503.875721	350856.862930	42.608128
3503.734817	350846.094422	42.613133
3503.605135	350841.661313	42.618138
3503.574451	350847.443655	42.623143
3503.702397	350831.746146	42.628148
3503.120447	350828.835214	42.633152
3503.586785	350814.483982	42.638157
3503.617052	350814.326721	42.643162
3503.261953	350826.599332	42.648167
3503.417450	350821.510326	42.653172
3503.441621	350836.268027	42.658176
3503.340345	350829.794386	42.663181
3503.625429	350829.571391	42.668186
3503.356645	350821.444497	42.673191
3503.702212	350804.007392	42.678196
3503.564833	350803.036767	42.683200
3503.934355	350799.135548	42.688205
3503.949003	350807.506681	42.693210
3503.791665	350802.085371	42.698215
3503.771097	350791.908641	42.703220
3503.697786	350793.523842	42.708224
3503.645544	350794.753953	42.713229
3503.568771	350775.754773	42.718234
3503.229252	350763.159759	42.723239
3503.627719	350758.923104	42.728244
3503.263174	350765.954411	42.733248
3503.684203	350771.054537	42.738253
3503.917414	350767.429370	42.743258
3503.652244	350756.349633	42.748263
3503.686243	350744.230026	42.753268
3503.774181	350744.369055	42.758272
3504.069402	350727.525247	42.763277
3504.014632	350728.170397	42.768282
3503.263084	350710.372243	42.773287
3503.893186	350705.869910	42.778292
3503.533331	350713.994856	42.783296
3503.608505	350709.503900	42.788301
3503.562399	350706.482799	42.793306
3503.684983	350690.709745	42.798311
3503.708632	350677.242879	42.803316
3503.536734	350684.421894	42.808321
3503.767422	350690.926450	42.813325
3503.753516	350686.424124	42.818330
3503.608935	350672.398489	42.823335
3503.674727	350654.369301	42.828340
3503.292612	350661.530652	42.833345
3503.310140	350664.276771	42.838349
3503.791909	350656.820166	42.843354
3503.536404	350656.326324	42.848359
3503.419642	350637.995132	42.853364
3503.727571	350635.325267	42.858369
3503.623212	350632.262471	42.863373
3503.826565	350634.139345	42.868378
3503.730365	350628.173890	42.873383
3503.972598	350602.048949	42.878388
3503.849860	350612.325177	42.883393
3503.621589	350610.936258	42.888397
3503.596084	350601.931000	42.893402
3503.360061	350593.366232	42.898407
3503.491551	350581.129374	42.903412
3503.385360	350580.840982	42.908417
3503.555123	350576.844074	42.913421
3503.555885	350581.654349	42.918426
3503.771800	350588.466660	42.923431
3503.911123	350569.407794	42.928436
3503.864361	350556.028381	42.933441
3503.708962	350555.238756	42.938445
3503.756453	350548.537957	42.943450
3503.802860	350542.219089	42.948455
3503.698051	350524.700390	42.953460
3503.552172	350527.777758	42.958465
3503.653505	350515.189343	42.963469
3503.694012	350524.116347	42.968474
3503.610473	350505.907111	42.973479
3503.569285	350484.713446	42.978484
3503.666843	350488.566753	42.983489
3503.817604	350487.499669	42.988493
3503.648816	350483.658079	42.993498
3503.460706	350480.710316	42.998503
3503.401032	350465.449572	43.003508
3503.802940	350467.982231	43.008513
3503.619803	350454.344395	43.013517
3503.476932	350461.697006	43.018522
3503.436973	350467.022743	43.023527
3503.714413	350463.874127	43.028532
3503.466848	350443.782001	43.033537
3503.437867	350445.721062	43.038541
3503.890737	350439.159769	43.043546
3503.645946	350446.401241	43.048551
3503.689629	350441.686185	43.053556
3503.621567	350434.087416	43.058561
3503.923023	350415.995441	43.063565
3503.629322	350417.238283	43.068570
3503.562884	350419.794084	43.073575
3503.245908	350417.197550	43.078580
3503.396303	350421.729677	43.083585
3503.646972	350396.697683	43.088589
3503.785353	350382.220028	43.093594
3503.700875	350382.462667	43.098599
3504.024678	350382.233549	43.103604
3503.645434	350382.522788	43.108609
3503.635728	350371.657093	43.113613
3503.900785	350367.085188	43.118618
3503.425722	350375.050243	43.123623
3503.659322	350364.527842	43.128628
3503.592353	350352.118701	43.133633
3503.727456	350331.253416	43.138637
3503.565316	350338.787245	43.143642
3503.400137	350330.109433	43.148647
3503.675139	350333.807444	43.153652
3503.191780	350351.190587	43.158657
3503.717271	350333.623084	43.163661
3503.782873	350319.665932	43.168666
3503.380095	350314.614235	43.173671
3503.635672	350304.851870	43.178676
3503.509176	350311.362038	43.183681
3503.639862	350302.866504	43.188685
3503.676943	350299.323215	43.193690
3503.627773	350287.700218	43.198695
3503.866006	350276.464447	43.203700
3503.453972	350285.437581	43.208705
3503.771372	350283.555176	43.213709
3503.837656	350260.995543	43.218714
3503.541485	350260.304519	43.223719
3503.809393	350246.366268	43.228724
3503.674776	350257.611571	43.233729
3503.708793	350259.973343	43.238733
3503.382224	350234.065401	43.243738
3503.393341	350225.079742	43.248743
3503.900986	350218.153452	43.253748
3503.748237	350222.809873	43.258753
3503.620285	350218.910906	43.263757
3504.098733	350198.194897	43.268762
3503.917229	350190.283167	43.273767
3503.772035	350187.277702	43.278772
3503.941462	350174.958403	43.283777
3503.488650	350153.626075	43.288781
3503.477864	350148.181531	43.293786
3503.449752	350152.589196	43.298791
3503.698232	350154.840716	43.303796
3503.426570	350158.014342	43.308801
3503.487511	350146.704769	43.313805
3503.525823	350131.835653	43.318810
3503.535810	350134.023074	43.323815
3503.862768	350126.489067	43.328820
3503.878542	350138.830456	43.333825
3503.679845	350129.216229	43.338829
3503.976498	350100.740967	43.343834
3503.796477	350095.628582	43.348839
3504.169849	350090.937727	43.353844
3503.513822	350074.116846	43.358849
3503.370408	350071.569208	43.363853
3503.465840	350068.551147	43.368858
3503.309130	350067.227253	43.373863
3503.447873	350067.969073	43.378868
3503.421818	350073.674413	43.383873
3503.862234	350066.427871	43.388877
3503.646825	350046.814081	43.393882
3503.641156	350046.229834	43.398887
3503.889655	350025.117448	43.403892
3503.413684	350037.612952	43.408897
3503.559021	350038.455533	43.413901
3503.655883	350030.118010	43.418906
3503.751594	350019.108324	43.423911
3504.042564	350008.704039	43.428916
3503.872417	350012.599701	43.433921
3503.465475	349996.197533	43.438925
3503.321846	349978.837501	43.443930
3502.962070	349988.107833	43.448935
3503.416269	349970.067916	43.453940
3503.369715	349987.280316	43.458945
3503.482560	349982.477934	43.463949
3503.784494	349988.258686	43.468954
3503.574627	350001.246599	43.473959
3503.595295	349979.050373	43.478964
3503.849014	349965.165195	43.483969
3503.524551	349961.297276	43.488973
3503.684309	349962.366637	43.493978
3503.752361	349965.512019	43.498983
3503.767640	349950.850103	43.503988
3503.567451	349931.513825	43.508993
3503.704056	349930.448969	43.513997
3503.873113	349918.689590	43.519002
3503.688855	349929.459241	43.524007
3503.672104	349927.375140	43.529012
3503.652706	349907.857567	43.534017
3503.425156	349908.530042	43.539021
3503.742508	349909.243627	43.544026
3503.481185	349909.997794	43.549031
3503.857653	349902.506830	43.554036
3503.685351	349890.114236	43.559041
3503.395513	349877.307554	43.564045
3503.606309	349876.103712	43.569050
3503.683813	349877.542392	43.574055
3503.601252	349874.883321	43.579060
3503.552826	349858.348081	43.584065
3503.200396	349852.703008	43.589069
3503.513352	349844.305843	43.594074
3503.400771	349849.286808	43.599079
3503.357952	349839.393377	43.604084
3503.273851	349846.634976	43.609089
3503.470867	349855.588248	43.614093
3503.428970	349850.606710	43.619098
3503.388418	349854.940013	43.624103
3503.539318	349849.877093	43.629108
3503.181736	349833.747034	43.634113
3503.262672	349826.200977	43.639117
3503.491064	349820.413176	43.644122
3503.338289	349832.679477	43.649127
3503.584282	349818.515522	43.654132
3503.527981	349827.788807	43.659137
3503.389731	349824.985832	43.664141
3503.602918	349830.882434	43.669146
3503.625859	349824.796252	43.674151
3503.701819	349802.082193	43.679156
3503.465565	349807.744438	43.684161
3503.400071	349802.563018	43.689165
3504.056415	349801.186934	43.694170
3503.603723	349799.858924	43.699175
3503.722325	349775.611053	43.704180
3503.504138	349772.820713	43.709185
3503.311873	349768.601018	43.714189
3503.398844	349765.787886	43.719194
3503.001901	349765.774513	43.724199
3503.101505	349772.834374	43.729204
3503.266069	349769.143641	43.734209
3503.522970	349778.189263	43.739213
3503.634072	349775.397767	43.744218
3503.385101	349762.482793	43.749223
3503.400281	349759.324696	43.754228
3503.694476	349744.033257	43.759233
3503.165788	349746.840324	43.764237
3503.457554	349754.149769	43.769242
3503.551069	349757.189334	43.774247
3503.499579	349746.559178	43.779252
3503.243504	349755.762254	43.784257
3503.520985	349753.809788	43.789261
3503.541694	349730.290002	43.794266
3503.309735	349727.552738	43.799271
3503.437581	349723.358787	43.804276
3503.160581	349728.314853	43.809281
3503.564839	349718.452526	43.814285
3503.932324	349715.111475	43.819290
3503.593377	349724.989384	43.824295
3503.932535	349704.015247	43.829300
3503.692638	349703.213516	43.834305
3503.706917	349694.481780	43.839309
3504.188079	349691.097305	43.844314
3503.712175	349668.801299	43.849319
3503.753254	349653.524399	43.854324
3503.546159	349656.636945	43.859329
3503.836643	349649.490404	43.864333
3503.662984	349647.354745	43.869338
3503.466621	349637.358297	43.874343
3503.779887	349621.554788	43.879348
3503.472811	349629.187981	43.884353
3503.300559	349628.706418	43.889357
3503.451006	349635.681905	43.894362
3503.672819	349632.923802	43.899367
3503.455425	349608.118149	43.904372
3503.372286	349598.765523	43.909377
3503.417800	349591.275936	43.914381
3503.297868	349591.625987	43.919386
3503.337887	349595.615709	43.924391
3503.404032	349591.558757	43.929396
3503.037157	349604.647939	43.934401
3503.367216	349601.872722	43.939405
3503.308965	349602.747495	43.944410
3502.915995	349604.286010	43.949415
3503.246269	349616.323287	43.954420
3503.552587	349606.629130	43.959425
3503.305999	349605.243080	43.964429
3503.308438	349593.637228	43.969434
3503.431280	349585.041019	43.974439
3503.409576	349578.478296	43.979444
3503.364444	349582.812344	43.984449
3503.327460	349583.632853	43.989453
3503.692754	349587.392995	43.994458
3503.542997	349593.194294	43.999463
3503.547311	349585.685769	44.004468
3503.367593	349588.946697	44.009473
3503.539118	349576.601479	44.014477
3503.321280	349562.561688	44.019482
3503.115883	349565.623068	44.024487
3503.572284	349555.599762	44.029492
3503.298266	349566.129163	44.034497
3503.272948	349562.519337	44.039501
3503.714474	349561.788035	44.044506
3503.313740	349569.410591	44.049511
3503.333989	349562.357663	44.054516
3503.359001	349569.531147	44.059521
3503.594142	349562.978719	44.064525
3503.663102	349547.086556	44.069530
3503.460055	349552.896284	44.074535
3503.629424	349533.094224	44.079540
3503.365405	349536.673895	44.084545
3503.500716	349537.568971	44.089549
3503.560291	349537.788841	44.094554
3503.347087	349528.711275	44.099559
3503.314016	349512.249856	44.104564
3503.485518	349527.060974	44.109569
3503.587335	349511.214508	44.114573
3503.899505	349512.208881	44.119578
3503.615407	349514.671878	44.124583
3503.737827	349504.192340	44.129588
3503.387582	349495.238238	44.134593
3503.374482	349483.838428	44.139597
3503.799739	349480.004658	44.144602
3503.266538	349485.866588	44.149607
3503.658129	349495.196377	44.154612
3503.496753	349491.480800	44.159617
3503.735215	349483.680733	44.164621
3503.520593	349463.506683	44.169626
3503.450282	349456.162644	44.174631
3503.562663	349445.124756	44.179636
3503.276048	349448.249885	44.184641
3503.130494	349464.714566	44.189645
3503.496884	349463.027997	44.194650
3503.407321	349470.346863	44.199655
3503.719487	349457.470362	44.204660
3503.480139	349445.113717	44.209665
3503.483028	349433.456857	44.214669
3503.747824	349424.863633	44.219674
3503.521732	349447.296623	44.224679
3503.775160	349423.129087	44.229684
3503.371611	349404.741014	44.234689
3503.598834	349393.786765	44.239693
3503.599644	349396.001117	44.244698
3503.345983	349399.655513	44.249703
3503.708302	349396.569771	44.254708
3503.518845	349405.126094	44.259713
3503.694948	349395.936058	44.264717
3503.548256	349381.325047	44.269722
3503.112938	349388.367719	44.274727
3503.425262	349379.665168	44.279732
3503.499727	349373.723497	44.284737
3503.230184	349388.197159	44.289741
3503.440491	349376.380240	44.294746
3503.611338	349377.676920	44.299751
3503.572274	349381.017429	44.304756
3503.577017	349365.288072	44.309761
3503.525912	349357.228350	44.314765
3503.663868	349344.023047	44.319770
3503.332522	349353.110833	44.324775
3503.377022	349345.265056	44.329780
3503.569021	349346.049369	44.334785
3503.464161	349346.269784	44.339789
3503.524653	349331.855066	44.344794
3503.277337	349329.680137	44.349799
3503.458971	349317.155105	44.354804
3503.387952	349322.867632	44.359809
3503.123491	349319.550108	44.364813
3503.502567	349321.348346	44.369818
3503.127152	349334.133528	44.374823
3503.253997	349330.194217	44.379828
3503.417802	349325.129209	44.384833
3503.542935	349329.461811	44.389837
3503.494185	349337.385071	44.394842
3503.214480	349311.749245	44.399847
3503.426854	349296.801483	44.404852
3503.495559	349302.110154	44.409857
3503.515617	349299.129418	44.414861
3503.442196	349302.806229	44.419866
3503.606962	349304.485640	44.424871
3503.563306	349298.384476	44.429876
3503.461039	349302.244006	44.434881
3503.346651	349279.687079	44.439885
3503.335673	349275.795003	44.444890
3503.376696	349278.893796	44.449895
3503.191294	349268.691938	44.454900
3503.394302	349283.701750	44.459905
3503.573688	349277.107201	44.464909
3503.530874	349272.253011	44.469914
3503.473689	349275.927257	44.474919
3503.653245	349277.273465	44.479924
3503.863914	349260.493474	44.484929
3503.758531	349244.476078	44.489933
3503.566761	349243.921243	44.494938
3503.417953	349247.024597	44.499943
3503.761034	349235.873842	44.504948
3503.399738	349222.849242	44.509953
3503.464826	349217.239903	44.514957
3503.469023	349206.753546	44.519962
3503.400896	349210.607685	44.524967
3503.554347	349204.831668	44.529972
3503.418993	349214.041200	44.534977
3503.368740	349214.151177	44.539981
3503.566822	349211.396805	44.544986
3503.320537	349195.045351	44.549991
3503.659487	349178.168701	44.554996
3503.440541	349185.991633	44.560001
3503.320155	349172.521715	44.565005
3503.762524	349169.881429	44.570010
3503.584096	349186.325939	44.575015
3503.534908	349183.559753	44.580020
3503.579777	349163.802694	44.585025
3503.623408	349147.812614	44.590029
3503.595990	349147.384504	44.595034
3503.237701	349158.818101	44.600039
3503.558569	349152.939257	44.605044
3503.305498	349167.054055	44.610049
3503.386927	349160.653136	44.615053
3503.331219	349165.243402	44.620058
3503.363409	349146.404587	44.625063
3503.426819	349131.353073	44.630068
3503.217758	349131.768121	44.635073
3503.460107	349131.322815	44.640077
3503.732184	349130.618296	44.645082
3503.132619	349136.745267	44.650087
3503.479188	349132.923913	44.655092
3503.309892	349136.794051	44.660097
3503.318600	349129.564733	44.665101
3503.341557	349132.284620	44.670106
3503.308673	349138.245650	44.675111
3503.404839	349129.068207	44.680116
3503.220545	349120.342321	44.685121
3503.272619	349113.004340	44.690125
3503.281642	349114.759281	44.695130
3503.227943	349111.892000	44.700135
3503.310949	349106.254366	44.705140
3503.371503	349110.037266	44.710145
3503.347148	349106.859930	44.715149
3503.382908	349121.718068	44.720154
3503.464948	349121.959839	44.725159
3503.822664	349111.341222	44.730164
3503.540468	349113.447618	44.735169
3503.574712	349082.035509	44.740173
3503.420377	349079.005976	44.745178
3503.100574	349081.958213	44.750183
3503.620741	349074.342614	44.755188
3503.254144	349076.920479	44.760193
3503.362814	349082.859137	44.765197
3503.355343	349088.790703	44.770202
3503.397143	349095.757984	44.775207
3503.422983	349086.540749	44.780212
3503.302081	349078.899242	44.785217
3503.443125	349067.322269	44.790221
3503.254569	349061.269437	44.795226
3503.150347	349060.522601	44.800231
3503.364862	349061.252456	44.805236
3503.385157	349060.435032	44.810241
3503.336171	349066.195005	44.815245
3503.653550	349073.169625	44.820250
3503.766237	349075.544462	44.825255
3503.379921	349063.847249	44.830260
3503.342802	349044.688489	44.835265
3503.252119	349035.413313	44.840269
3503.530985	349032.620709	44.845274
3503.457873	349034.566797	44.850279
3503.846686	349031.705909	44.855284
3503.202793	349043.184681	44.860289
3503.077299	349034.933061	44.865293
3503.288072	349037.546907	44.870298
3503.438261	349048.696530	44.875303
3503.983166	349031.354603	44.880308
3503.746634	349015.994157	44.885313
3503.762578	349007.262049	44.890317
3503.981375	348998.981446	44.895322
3503.247516	349005.485982	44.900327
3503.655560	348974.116521	44.905332
3503.720431	348971.357745	44.910337
3503.808110	348961.163561	44.915341
3503.422120	348971.049041	44.920346
3503.617530	348972.341848	44.925351
3503.569876	348957.791421	44.930356
3503.365464	348946.116328	44.935361
3503.157545	348947.956474	44.940365
3503.657455	348941.387567	44.945370
3503.385907	348942.499682	44.950375
3503.603148	348944.145358	44.955380
3503.475672	348950.248619	44.960385
3503.550665	348951.076887	44.965389
3503.577209	348929.439238	44.970394
3503.621985	348919.913564	44.975399
3503.768677	348907.979346	44.980404
3503.473550	348905.710152	44.985409
3503.617268	348907.112938	44.990413
3503.612762	348898.460400	44.995418
3503.202547	348887.021441	45.000423
3503.331322	348863.127880	45.005428
3502.996267	348871.529144	45.010433
3503.447167	348873.621459	45.015437
3503.194897	348870.123820	45.020442
3503.283259	348877.185573	45.025447
3503.324790	348878.884480	45.030452
3503.147416	348877.334761	45.035457
3503.352700	348884.479834	45.040461
3503.655658	348885.552029	45.045466
3503.374788	348883.127873	45.050471
3503.690997	348888.092039	45.055476
3503.901494	348877.878423	45.060481
3503.583033	348861.767344	45.065485
3503.486952	348849.947847	45.070490
3503.521624	348856.992639	45.075495
3503.780635	348846.440479	45.080500
3503.689024	348839.201531	45.085505
3503.432205	348827.458344	45.090509
3503.628134	348822.286405	45.095514
3503.324359	348821.138439	45.100519
3503.601368	348819.898657	45.105524
3503.421106	348810.739410	45.110529
3503.517571	348816.247351	45.115533
3503.718895	348799.748664	45.120538
3503.331540	348792.149240	45.125543
3503.551593	348773.764176	45.130548
3503.375897	348787.332358	45.135553
3503.040606	348790.414315	45.140557
3503.460784	348786.072271	45.145562
3503.370966	348785.577669	45.150567
3503.275616	348791.574064	45.155572
3503.380824	348788.248969	45.160577
3503.486870	348789.963131	45.165581
3503.528786	348779.725245	45.170586
3503.025332	348765.119569	45.175591
3503.530652	348750.354410	45.180596
3503.102719	348761.977259	45.185601
3503.173722	348764.435054	45.190605
3503.245444	348757.602949	45.195610
3503.326376	348765.200371	45.200615
3503.285459	348760.625803	45.205620
3502.962246	348763.069566	45.210625
3503.305918	348761.742888	45.215629
3503.592564	348764.192044	45.220634
3503.945160	348772.051936	45.225639
3503.990290	348761.991699	45.230644
3503.742697	348735.637887	45.235649
3503.663467	348738.653915	45.240653
3503.642549	348731.531035	45.245658
3503.656518	348733.361561	45.250663
3503.535821	348719.102585	45.255668
3503.500771	348710.683910	45.260673
3503.371022	348703.832746	45.265677
3503.544398	348702.558441	45.270682
3503.489636	348716.438390	45.275687
3503.581886	348701.840327	45.280692
3503.789024	348696.717509	45.285697
3503.147872	348680.708294	45.290701
3503.673620	348669.681256	45.295706
3503.380661	348672.960140	45.300711
3503.494592	348661.463724	45.305716
3503.135700	348668.138083	45.310721
3503.490416	348672.154475	45.315725
3503.502233	348665.891762	45.320730
3503.385659	348673.138649	45.325735
3503.556151	348669.294196	45.330740
3503.551001	348645.218101	45.335745
3503.309888	348650.677621	45.340749
3503.244606	348637.606085	45.345754
3503.599172	348633.019887	45.350759
3503.658432	348638.762792	45.355764
3503.381877	348641.784569	45.360769
3503.723143	348644.734125	45.365773
3503.762952	348618.767498	45.370778
3503.413619	348616.634120	45.375783
3503.686507	348602.083829	45.380788
3503.484762	348610.336798	45.385793
3503.409012	348604.927823	45.390797
3503.676589	348595.901354	45.395802
3503.505919	348581.039406	45.400807
3503.404886	348584.924242	45.405812
3503.332774	348580.939976	45.410817
3503.405097	348582.659476	45.415821
3503.524327	348576.379772	45.420826
3503.308520	348588.910829	45.425831
3503.196377	348584.398409	45.430836
3503.271432	348585.761155	45.435841
3503.294197	348590.033644	45.440845
3503.511226	348581.905968	45.445850
3503.531882	348579.281420	45.450855
3503.339549	348552.460657	45.455860
3503.204704	348551.438689	45.460865
3503.171325	348553.734834	45.465869
3503.007512	348545.514651	45.470874
3502.845219	348553.914102	45.475879
3503.299541	348557.125757	45.480884
3503.470845	348548.267209	45.485889
3503.300101	348554.962740	45.490893
3503.212927	348552.355238	45.495898
3503.135662	348561.224825	45.500903
3503.377451	348556.580095	45.505908
3503.225026	348563.272729	45.510913
3503.399239	348558.206006	45.515917
3503.470826	348545.901809	45.520922
3503.205467	348554.037586	45.525927
3503.254906	348553.215548	45.530932
3503.221697	348557.776856	45.535937
3503.412454	348562.964497	45.540941
3503.494981	348556.792399	45.545946
3503.263845	348550.288115	45.550951
3503.379859	348529.959647	45.555956
3503.349266	348534.342382	45.560961
3503.094178	348534.484743	45.565965
3503.338070	348520.346239	45.570970
3503.044934	348537.139947	45.575975
3503.187111	348528.260549	45.580980
3503.359856	348532.356623	45.585985
3503.147453	348543.512767	45.590989
3503.172006	348543.814532	45.595994
3503.547247	348537.545253	45.600999
3503.295487	348535.167382	45.606004
3503.614813	348542.345374	45.611009
3503.381218	348546.505685	45.616013
3503.735268	348530.084579	45.621018
3503.520814	348507.135932	45.626023
3503.636266	348503.427427	45.631028
3503.962845	348503.401477	45.636033
3503.414741	348497.787198	45.641037
3503.501490	348501.616902	45.646042
3503.299734	348485.919941	45.651047
3503.496990	348473.061377	45.656052
3503.245832	348476.079148	45.661057
3503.302802	348474.568725	45.666061
3503.418264	348472.107345	45.671066
3502.927955	348474.170311	45.676071
3503.041422	348479.777405	45.681076
3503.290003	348475.564271	45.686081
3503.482422	348481.387947	45.691085
3503.594420	348475.974729	45.696090
3503.218976	348488.174724	45.701095
3503.593432	348473.633793	45.706100
3503.469320	348488.517376	45.711105
3503.368333	348467.103321	45.716109
3503.714733	348445.873046	45.721114
3503.354274	348449.875259	45.726119
3503.477094	348445.096618	45.731124
3503.605199	348444.923883	45.736129
3503.177394	348451.940034	45.741133
3503.272451	348444.442459	45.746138
3503.032425	348452.039762	45.751143
3503.613778	348458.310986	45.756148
3503.343846	348444.991791	45.761153
3503.055638	348441.703419	45.766157
3503.399841	348423.171354	45.771162
3503.157823	348418.017711	45.776167
3503.048757	348411.366854	45.781172
3503.411595	348418.843402	45.786177
3503.407783	348419.862298	45.791181
3503.630867	348424.637615	45.796186
3503.031100	348431.706405	45.801191
3503.125777	348426.677696	45.806196
3503.471543	348425.961518	45.811201
3503.180511	348430.105467	45.816205
3503.050777	348435.216529	45.821210
3503.347163	348434.889932	45.826215
3503.116718	348433.017720	45.831220
3503.450362	348440.575235	45.836225
3503.414847	348443.584368	45.841229
3503.561783	348432.540815	45.846234
3503.075108	348425.313366	45.851239
3503.460960	348415.580976	45.856244
3503.335581	348398.955657	45.861249
3503.264627	348405.202752	45.866253
3503.378333	348395.309769	45.871258
3503.166606	348404.811477	45.876263
3503.554531	348399.507340	45.881268
3503.657621	348402.545467	45.886273
3503.526445	348403.533594	45.891277
3503.702279	348406.102091	45.896282
3503.588793	348394.794281	45.901287
3503.502837	348380.249758	45.906292
3503.984333	348375.719828	45.911297
3503.348628	348379.841915	45.916301
3503.324456	348373.864827	45.921306
3503.201641	348374.800730	45.926311
3503.553424	348373.167341	45.931316
3503.370423	348356.805635	45.936321
3503.327062	348345.843053	45.941325
3503.560983	348336.720056	45.946330
3503.365209	348343.495925	45.951335
3503.539134	348336.342190	45.956340
3503.463962	348337.626885	45.961345
3503.386080	348343.646018	45.966349
3503.506008	348346.401517	45.971354
3503.460406	348331.265214	45.976359
3503.433296	348312.079166	45.981364
3503.252243	348316.103930	45.986369
3503.377810	348308.423352	45.991373
3503.445120	348310.169104	45.996378
3503.107847	348310.578975	46.001383
3503.158790	348317.570360	46.006388
3503.537442	348317.485274	46.011393
3503.309101	348323.146420	46.016397
3503.470591	348306.450270	46.021402
3503.548322	348314.480939	46.026407
3503.793371	348304.898047	46.031412
3503.429854	348293.349777	46.036417
3503.231527	348283.811524	46.041421
3503.517435	348269.717217	46.046426
3503.494025	348284.661289	46.051431
3503.518812	348278.930968	46.056436
3503.804498	348280.311326	46.061441
3503.661346	348267.277465	46.066445
3503.302095	348252.419791	46.071450
3503.341578	348259.743867	46.076455
3503.725534	348255.407508	46.081460
3503.400605	348252.252190	46.086465
3502.756460	348262.229512	46.091469
3503.296722	348251.912744	46.096474
3502.866736	348253.406244	46.101479
3503.036328	348255.339442	46.106484
3503.294381	348248.757786	46.111489
3503.299413	348255.298306	46.116493
3503.679391	348256.358337	46.121498
3502.943271	348263.143284	46.126503
3503.491546	348258.348270	46.131508
3503.140768	348261.559963	46.136513
3502.916334	348256.887107	46.141517
3503.468375	348248.910034	46.146522
3503.400225	348265.413738	46.151527
3503.461084	348247.919025	46.156532
3503.333497	348235.900765	46.161537
3503.015525	348233.558800	46.166541
3503.310807	348219.768420	46.171546
3503.012181	348229.742027	46.176551
3503.403157	348232.429230	46.181556
3503.353169	348232.768232	46.186561
3503.499389	348224.702602	46.191565
3503.592361	348223.517352	46.196570
3503.307467	348234.761373	46.201575
3503.322036	348230.636120	46.206580
3503.691497	348221.771646	46.211585
3503.378215	348217.367350	46.216589
3503.516522	348206.783247	46.221594
3503.424059	348200.206096	46.226599
3503.525182	348194.870925	46.231604
3503.482633	348199.077415	46.236609
3502.843291	348196.099058	46.241613
3503.333753	348189.964235	46.246618
3503.487274	348197.957488	46.251623
3503.228095	348203.038131	46.256628
3503.343099	348201.900302	46.261633
3503.424750	348200.207807	46.266637
3503.709111	348191.611298	46.271642
3503.334638	348182.788072	46.276647
3503.662522	348166.905482	46.281652
3503.724543	348170.357342	46.286657
3503.565486	348171.960723	46.291661
3503.732017	348173.487179	46.296666
3503.435790	348160.273880	46.301671
3503.247327	348143.989330	46.306676
3502.995059	348140.491646	46.311681
3502.962426	348140.395225	46.316685
3503.371785	348140.457995	46.321690
3503.064818	348147.302370	46.326695
3503.114904	348135.408710	46.331700
3503.449587	348144.544111	46.336705
3503.126094	348152.460071	46.341709
3503.471418	348141.690518	46.346714
3503.186766	348151.305605	46.351719
3503.745404	348151.624745	46.356724
3503.576831	348148.724671	46.361729
3503.352957	348150.770980	46.366733
3503.544395	348141.680119	46.371738
3503.310067	348128.660640	46.376743
3503.501559	348113.181374	46.381748
3503.505034	348118.296857	46.386753
3503.526044	348111.981725	46.391757
3503.519706	348114.935360	46.396762
3503.294542	348112.629621	46.401767
3503.298124	348119.475808	46.406772
3503.387363	348110.070225	46.411777
3503.364208	348112.644742	46.416781
3503.438709	348114.847496	46.421786
3503.125358	348096.673793	46.426791
3503.489317	348082.897974	46.431796
3503.399996	348091.744090	46.436801
3503.133553	348085.754368	46.441805
3503.594048	348084.027430	46.446810
3503.553560	348074.387833	46.451815
3503.598803	348079.293102	46.456820
3503.482079	348092.444901	46.461825
3503.542023	348077.597264	46.466829
3503.429779	348061.886032	46.471834
3503.292102	348058.217515	46.476839
3503.502078	348054.468586	46.481844
3503.270934	348052.392856	46.486849
3503.079318	348057.284669	46.491853
3503.397396	348052.475126	46.496858
3503.245518	348059.600415	46.501863
3503.457973	348047.681067	46.506868
3503.529442	348055.738215	46.511873
3503.663570	348056.531695	46.516877
3503.967397	348027.901520	46.521882
3503.612403	348028.670519	46.526887
3503.779492	348023.044934	46.531892
3504.015457	348014.608760	46.536897
3503.995409	348006.798450	46.541901
3503.998500	347980.328295	46.546906
3503.606135	347978.430761	46.551911
3503.693495	347968.720031	46.556916
3503.471898	347962.901369	46.561921
3503.182834	347955.235388	46.566925
3503.544289	347945.252255	46.571930
3503.024325	347955.668132	46.576935
3503.119609	347949.086721	46.581940
3503.140561	347938.444765	46.586945
3503.120907	347948.959712	46.591949
3503.434821	347944.150818	46.596954
3503.315298	347948.929435	46.601959
3503.410542	347949.347287	46.606964
3503.537144	347952.712595	46.611969
3503.347541	347955.186174	46.616973
3503.990957	347944.369457	46.621978
3503.648676	347935.337487	46.626983
3503.502032	347930.117817	46.631988
3503.497489	347916.476570	46.636993
3503.055972	347913.365115	46.641997
3503.372534	347917.158527	46.647002
3503.258817	347920.078244	46.652007
3503.534943	347912.602876	46.657012
3503.421349	347897.044523	46.662017
3503.558185	347893.103530	46.667021
3503.476505	347876.496599	46.672026
3503.311529	347885.176545	46.677031
3503.409637	347885.670300	46.682036
3503.583648	347886.584737	46.687041
3503.222541	347882.111619	46.692045
3503.449692	347880.090690	46.697050
3503.166338	347881.433759	46.702055
3503.465620	347884.288186	46.707060
3503.291788	347863.496260	46.712065
3503.403324	347848.691310	46.717069
3503.491633	347833.126472	46.722074
3503.122899	347845.885487	46.727079
3503.375508	347847.551056	46.732084
3503.113751	347840.771559	46.737089
3503.138298	347850.541431	46.742093
3503.155951	347857.512684	46.747098
3503.144888	347856.903815	46.752103
3503.743933	347847.086719	46.757108
3503.594772	347853.880729	46.762113
3503.691032	347851.498713	46.767117
3503.498620	347829.844349	46.772122
3503.238634	347824.795298	46.777127
3503.107206	347820.489481	46.782132
3502.943191	347821.406454	46.787137
3503.389046	347819.783630	46.792141
3503.583714	347816.520691	46.797146
3503.190991	347822.106067	46.802151
3503.386494	347815.686960	46.807156
3503.190420	347819.765037	46.812161
3503.041689	347827.169829	46.817165
3503.116301	347827.310972	46.822170
3502.994900	347828.628439	46.827175
3503.077545	347824.797816	46.832180
3503.062824	347820.269933	46.837185
3503.080426	347827.317554	46.842189
3503.122297	347833.546877	46.847194
3503.129705	347835.225758	46.852199
3503.495464	347826.921748	46.857204
3503.477526	347822.852508	46.862209
3503.247658	347836.505840	46.867213
3503.737772	347827.113191	46.872218
3503.387626	347830.630232	46.877223
3503.639051	347818.322896	46.882228
3503.283188	347814.103463	46.887233
3503.196386	347798.948077	46.892237
3503.326090	347795.720859	46.897242
3503.192428	347794.800496	46.902247
3503.190688	347794.571932	46.907252
3503.458502	347799.060260	46.912257
3503.318235	347799.948028	46.917261
3503.296084	347801.631583	46.922266
3502.809654	347801.606904	46.927271
3503.207886	347798.973532	46.932276
3503.520579	347803.582024	46.937281
3503.441351	347797.766290	46.942285
3503.674940	347794.191773	46.947290
3503.231188	347788.789993	46.952295
3503.168688	347781.597209	46.957300
3503.693430	347773.980711	46.962305
3503.624508	347777.147873	46.967309
3503.432608	347773.640621	46.972314
3503.707926	347773.699131	46.977319
3503.407326	347785.403860	46.982324
3503.336518	347786.382454	46.987329
3503.129795	347783.259325	46.992333
3503.498337	347774.522185	46.997338
3503.050894	347765.252294	47.002343
3503.236316	347753.922552	47.007348
3503.339169	347745.965516	47.012353
3503.135422	347740.856664	47.017357
3503.547392	347741.377157	47.022362
3503.417337	347744.452177	47.027367
3503.010046	347749.403565	47.032372
3503.375779	347745.553636	47.037377
3503.320342	347746.580705	47.042381
3503.486980	347741.006066	47.047386
3503.011199	347753.858381	47.052391
3503.162675	347746.657217	47.057396
3503.354375	347744.107397	47.062401
3502.942468	347749.746717	47.067405
3503.620298	347748.596256	47.072410
3503.280061	347757.914775	47.077415
3503.398749	347747.410044	47.082420
3503.483316	347728.053429	47.087425
3503.083451	347721.753886	47.092429
3503.558421	347716.385020	47.097434
3503.445019	347725.133193	47.102439
3503.536049	347714.276501	47.107444
3503.701881	347715.599465	47.112449
3503.764494	347728.875709	47.117453
3503.599621	347714.063518	47.122458
3503.613345	347700.495685	47.127463
3503.553001	347691.928143	47.132468
3503.528339	347693.001252	47.137473
3503.469211	347695.835995	47.142477
3503.671203	347684.630879	47.147482
3503.136714	347681.101426	47.152487
3502.915454	347663.422064	47.157492
3503.457781	347664.481893	47.162497
3502.954519	347672.299080	47.167501
3503.131681	347675.376440	47.172506
3503.334944	347671.704902	47.177511
3503.511654	347660.961914	47.182516
3503.565625	347659.579203	47.187521
3503.335317	347660.023072	47.192525
3503.495982	347653.405838	47.197530
3503.491235	347663.409442	47.202535
3503.463092	347655.880334	47.207540
3503.645991	347663.512691	47.212545
3503.318439	347650.456935	47.217549
3503.278221	347625.902357	47.222554
3503.005312	347629.712624	47.227559
3502.932673	347622.114191	47.232564
3503.378420	347624.436436	47.237569
3503.160274	347624.114823	47.242573
3503.380899	347618.735254	47.247578
3503.347921	347626.732620	47.252583
3503.310089	347624.422697	47.257588
3503.462647	347628.827452	47.262593
3503.210345	347634.212484	47.267597
3503.504013	347628.541396	47.272602
3503.251419	347632.475711	47.277607
3503.463773	347632.060587	47.282612
3503.441766	347634.787656	47.287617
3502.752326	347642.125242	47.292621
3503.190880	347632.638903	47.297626
3503.190142	347637.831453	47.302631
3503.265209	347634.129275	47.307636
3503.360350	347641.011949	47.312641
3503.146765	347635.039275	47.317645
3503.252182	347630.136055	47.322650
3502.841597	347617.373390	47.327655
3503.318001	347628.751698	47.332660
3503.523035	347629.966659	47.337665
3503.039585	347618.488113	47.342669
3503.366618	347608.306745	47.347674
3503.424748	347610.715723	47.352679
3503.473656	347603.759823	47.357684
3503.446548	347607.276712	47.362689
3503.417359	347610.793930	47.367693
3503.371738	347607.670774	47.372698
3502.975365	347616.896383	47.377703
3503.591595	347606.898364	47.382708
3503.497410	347607.346165	47.387713
3503.228036	347624.721785	47.392717
3503.110683	347619.904687	47.397722
3503.311412	347613.764703	47.402727
3503.154207	347594.904401	47.407732
3503.419149	347586.081802	47.412737
3503.311598	347579.659675	47.417741
3503.540067	347574.380669	47.422746
3503.535104	347572.727300	47.427751
3503.535586	347568.502418	47.432756
3503.535597	347570.666064	47.437761
3503.632366	347578.235693	47.442765
3503.447185	347558.870761	47.447770
3503.404337	347551.547581	47.452775
3503.230500	347549.055541	47.457780
3503.233393	347542.437785	47.462785
3503.186058	347550.742855	47.467789
3503.417303	347537.471472	47.472794
3502.973305	347546.322841	47.477799
3503.191766	347543.590617	47.482804
3503.390720	347550.864122	47.487809
3503.355644	347555.731231	47.492813
3503.521346	347547.789684	47.497818
3503.508720	347543.872296	47.502823
3503.587789	347553.659052	47.507828
3503.615837	347539.834396	47.512833
3503.289258	347517.106685	47.517837
3503.435501	347507.742894	47.522842
3503.275234	347520.010889	47.527847
3503.422479	347512.912172	47.532852
3503.682495	347515.340141	47.537857
3503.304523	347524.435595	47.542861
3503.175609	347517.584154	47.547866
3503.023262	347525.422241	47.552871
3503.197471	347523.511477	47.557876
3503.165185	347524.153110	47.562881
3503.266321	347525.104526	47.567885
3503.339955	347521.682540	47.572890
3502.805199	347533.068010	47.577895
3503.249304	347528.416663	47.582900
3503.528000	347525.878532	47.587905
3502.887119	347518.929864	47.592909
3503.358443	347521.604399	47.597914
3503.328479	347503.589319	47.602919
3503.331262	347490.201330	47.607924
3503.376160	347485.536735	47.612929
3503.155883	347487.811567	47.617933
3503.463204	347485.421621	47.622938
3503.437281	347497.235697	47.627943
3503.416944	347490.494347	47.632948
3503.565265	347487.442333	47.637953
3503.537719	347500.452911	47.642957
3503.354378	347497.224262	47.647962
3503.304958	347491.658304	47.652967
3503.257304	347471.431683	47.657972
3503.272427	347455.114748	47.662977
3502.827897	347452.156456	47.667981
3503.344963	347455.536421	47.672986
3503.302368	347459.183027	47.677991
3503.226634	347462.580352	47.682996
3503.823724	347450.676427	47.688001
3503.367748	347460.013292	47.693005
3503.496292	347452.866620	47.698010
3503.378441	347465.204278	47.703015
3503.474051	347465.698431	47.708020
3503.550761	347460.137982	47.713025
3503.234724	347446.036824	47.718029
3503.328358	347436.910407	47.723034
3503.276480	347438.853193	47.728039
3503.132230	347428.746300	47.733044
3503.218241	347436.215840	47.738049
3503.278826	347434.272132	47.743053
3503.608229	347426.177427	47.748058
3503.328226	347435.690094	47.753063
3503.483434	347431.033506	47.758068
3503.568776	347433.209121	47.763073
3503.383419	347438.710847	47.768077
3503.505735	347417.032020	47.773082
3503.310982	347400.188303	47.778087
3503.251587	347400.274277	47.783092
3503.460475	347388.711683	47.788097
3503.039955	347397.941145	47.793101
3503.375869	347392.594232	47.798106
3503.138065	347399.351407	47.803111
3503.236383	347395.111044	47.808116
3503.356029	347388.831141	47.813121
3503.175327	347398.633540	47.818125
3503.259645	347393.530019	47.823130
3503.112595	347404.065208	47.828135
3503.081071	347396.612956	47.833140
3503.473258	347396.831155	47.838145
3502.961699	347393.883457	47.843149
3503.433634	347403.200897	47.848154
3503.136370	347414.268873	47.853159
3503.422371	347398.138167	47.858164
3503.204608	347403.543212	47.863169
3503.103312	347409.718859	47.868173
3503.385926	347411.965095	47.873178
3503.594438	347413.586744	47.878183
3503.114694	347392.079444	47.883188
3503.051846	347381.628796	47.888193
3502.567931	347379.058508	47.893197
3503.019960	347392.044199	47.898202
3503.211899	347405.529143	47.903207
3503.082894	347405.753382	47.908212
3503.495339	347407.444600	47.913217
3503.530526	347402.985149	47.918221
3503.538601	347381.578889	47.923226
3503.228457	347379.362911	47.928231
3503.339745	347375.654990	47.933236
3503.552584	347371.981919	47.938241
3503.507363	347374.559958	47.943245
3503.674468	347380.260490	47.948250
3503.523556	347378.986519	47.953255
3503.348125	347361.248912	47.958260
3503.471755	347351.455985	47.963265
3503.219622	347356.586495	47.968269
3503.309179	347341.021323	47.973274
3503.390533	347341.670444	47.978279
3502.898935	347340.017645	47.983284
3503.423955	347335.760724	47.988289
3503.701113	347345.643461	47.993293
3503.807056	347341.834574	47.998298
3503.385286	347345.388420	48.003303
3503.402691	347337.597549	48.008308
3503.613166	347313.537697	48.013313
3502.947121	347315.704843	48.018317
3502.970444	347309.669229	48.023322
3503.167744	347311.878052	48.028327
3503.271037	347322.806365	48.033332
3503.535280	347322.612105	48.038337
3503.090014	347323.293577	48.043341
3503.410177	347326.042923	48.048346
3503.293523	347327.105129	48.053351
3503.322864	347320.152288	48.058356
3503.069922	347318.309047	48.063361
3503.052886	347336.841113	48.068365
3503.261379	347327.136574	48.073370
3503.300137	347327.359743	48.078375
3503.197249	347320.809588	48.083380
3503.505157	347332.036429	48.088385
3503.363329	347326.459611	48.093389
3503.301929	347327.691247	48.098394
3503.467190	347315.371972	48.103399
3503.269052	347299.241420	48.108404
3503.512997	347290.065764	48.113409
3503.201965	347291.718648	48.118413
3502.947465	347291.606397	48.123418
3503.172328	347290.527538	48.128423
3503.064522	347296.475157	48.133428
3503.263649	347285.194059	48.138433
3503.412943	347295.173375	48.143437
3503.309688	347291.702983	48.148442
3503.292094	347291.527827	48.153447
3503.352794	347290.042235	48.158452
3503.341139	347290.960582	48.163457
3503.218265	347296.401540	48.168461
3503.350726	347297.195295	48.173466
3503.380236	347307.015381	48.178471
3503.366482	347302.283687	48.183476
3503.128472	347304.306808	48.188481
3503.072337	347305.130378	48.193485
3503.645402	347289.259684	48.198490
3503.035700	347276.070282	48.203495
3503.000475	347272.334613	48.208500
3503.182733	347255.074920	48.213505
3503.092390	347273.669501	48.218509
3503.184072	347264.976051	48.223514
3503.215566	347262.960580	48.228519
3503.229000	347264.969404	48.233524
3503.179633	347267.522651	48.238529
3503.198999	347266.221757	48.243533
3503.458354	347264.602950	48.248538
3503.086295	347271.050486	48.253543
3503.577222	347261.683067	48.258548
3503.684357	347270.574610	48.263553
3503.418410	347271.405899	48.268557
3503.459129	347263.611331	48.273562
3503.472952	347276.386352	48.278567
3503.447420	347257.963259	48.283572
3503.626712	347249.612287	48.288577
3502.937201	347240.660552	48.293581
3502.993022	347227.645899	48.298586
3503.150945	347242.841554	48.303591
3503.292901	347237.448933	48.308596
3503.696524	347229.800606	48.313601
3503.442297	347236.840370	48.318605
3503.598698	347236.052307	48.323610
3503.217774	347231.964053	48.328615
3503.413629	347242.037826	48.333620
3503.307993	347241.545711	48.338625
3503.073939	347241.990175	48.343629
3503.611488	347239.563822	48.348634
3503.132722	347224.775674	48.353639
3503.127742	347217.471915	48.358644
3503.292314	347217.547934	48.363649
3503.361811	347221.024122	48.368653
3503.593980	347215.184551	48.373658
3503.456139	347219.966126	48.378663
3503.417282	347219.208931	48.383668
3503.360492	347221.025241	48.388673
3503.410273	347227.253380	48.393677
3503.609368	347218.542942	48.398682
3503.497979	347219.197084	48.403687
3503.030672	347198.400404	48.408692
3503.564880	347183.375746	48.413697
3503.125747	347186.117877	48.418701
3503.335874	347184.659562	48.423706
3503.334431	347182.089347	48.428711
3503.232358	347178.720570	48.433716
3503.448796	347180.315521	48.438721
3503.150665	347180.082907	48.443725
3503.262938	347172.989676	48.448730
3503.410099	347186.201777	48.453735
3503.187716	347178.423339	48.458740
3503.536927	347183.204275	48.463745
3503.396259	347187.222735	48.468749
3503.341288	347176.821708	48.473754
3503.274862	347166.117063	48.478759
3503.229253	347146.577212	48.483764
3503.273561	347145.959582	48.488769
3503.136973	347155.780501	48.493773
3503.476655	347149.771212	48.498778
3503.416599	347154.642305	48.503783
3503.142612	347155.042178	48.508788
3503.508639	347148.850559	48.513793
3503.248166	347147.695712	48.518797
3503.635978	347146.972872	48.523802
3503.337179	347158.473828	48.528807
3503.435098	347154.208058	48.533812
3503.493861	347124.750792	48.538817
3503.092610	347122.447398	48.543821
3503.044155	347114.157863	48.548826
3503.227727	347114.459948	48.553831
3503.270468	347111.170083	48.558836
3503.328151	347112.993751	48.563841
3503.173968	347127.398856	48.568845
3503.223564	347119.399247	48.573850
3503.073851	347118.201437	48.578855
3503.068714	347109.243295	48.583860
3503.262958	347112.928838	48.588865
3502.989711	347123.560386	48.593869
3502.986877	347116.790773	48.598874
3502.750229	347122.427900	48.603879
3502.890159	347118.842696	48.608884
3502.982772	347142.167960	48.613889
3502.728241	347155.978068	48.618893
3503.352386	347164.889702	48.623898
3503.384199	347168.066425	48.628903
3503.302259	347167.621467	48.633908
3503.487444	347159.804046	48.638913
3502.796613	347154.746692	48.643917
3503.205483	347149.235509	48.648922
3502.785717	347166.787759	48.653927
3503.232796	347165.826480	48.658932
3503.557686	347163.306482	48.663937
3503.239029	347153.176207	48.668941
3503.264043	347137.010330	48.673946
3503.079273	347144.777239	48.678951
3503.443187	347141.156626	48.683956
3503.582036	347131.641229	48.688961
3503.238318	347144.345543	48.693965
3502.965788	347143.167149	48.698970
3503.074138	347140.757740	48.703975
3503.422398	347145.716995	48.708980
3503.488530	347143.568783	48.713985
3503.270157	347142.330923	48.718989
3503.284074	347132.886181	48.723994
3503.015693	347148.760110	48.728999
3502.742115	347150.432530	48.734004
3503.637197	347146.193447	48.739009
3503.352120	347146.366004	48.744013
3503.745979	347150.987171	48.749018
3503.457270	347148.462369	48.754023
3503.279310	347127.619920	48.759028
3503.503444	347120.076310	48.764033
3503.261177	347115.304369	48.769037
3503.430157	347110.594674	48.774042
3503.384742	347126.713335	48.779047
3503.255863	347122.330704	48.784052
3503.485296	347114.328116	48.789057
3503.258828	347124.723198	48.794061
3503.321621	347121.328354	48.799066
3503.316852	347114.966282	48.804071
3503.760563	347106.497129	48.809076
3503.708334	347091.310635	48.814081
3503.536566	347088.207393	48.819085
3503.750867	347073.487803	48.824090
3503.616486	347081.857608	48.829095
3503.316154	347084.959584	48.834100
3503.380037	347068.558472	48.839105
3503.264563	347055.850834	48.844109
3503.289499	347047.371521	48.849114
3503.303335	347057.601365	48.854119
3502.942927	347045.136064	48.859124
3503.344099	347040.567821	48.864129
3503.042110	347048.073300	48.869133
3503.222456	347047.586876	48.874138
3503.214189	347047.155722	48.879143
3503.085577	347054.353816	48.884148
3503.396684	347050.639737	48.889153
3503.194560	347044.334309	48.894157
3503.708610	347042.191637	48.899162
3503.821177	347044.744746	48.904167
3503.641962	347042.202628	48.909172
3503.416531	347020.120484	48.914177
3503.458495	347021.793927	48.919181
3503.614136	347008.279849	48.924186
3503.257244	347006.885719	48.929191
3503.383964	347006.916818	48.934196
3503.470386	347003.670945	48.939201
3503.394067	347001.647056	48.944205
3503.464984	347007.388285	48.949210
3503.362433	347011.680706	48.954215
3503.185241	346993.459669	48.959220
3503.467625	346983.437962	48.964225
3503.426596	346984.080983	48.969229
3503.644217	346976.945621	48.974234
3503.481627	346976.335246	48.979239
3503.237365	346979.631981	48.984244
3503.692468	346970.931937	48.989249
3503.182360	346976.510502	48.994253
3503.503136	346973.914789	48.999258
3503.331131	346957.296414	49.004263
3503.209599	346937.997564	49.009268
3503.361542	346942.071591	49.014273
3502.980106	346943.175665	49.019277
3503.521665	346935.301873	49.024282
3503.438256	346938.344110	49.029287
3503.202464	346951.514999	49.034292
3503.451158	346950.279652	49.039297
3503.256083	346954.739418	49.044301
3503.345926	346944.417264	49.049306
3503.092804	346942.217706	49.054311
3502.882976	346946.323473	49.059316
3503.222983	346944.233764	49.064321
3503.054833	346946.373116	49.069325
3503.481496	346945.440513	49.074330
3503.185309	346946.047516	49.079335
3503.178675	346951.342869	49.084340
3503.547959	346943.369053	49.089345
3503.369111	346952.254953	49.094349
3503.164061	346936.507174	49.099354
3503.152818	346932.385907	49.104359
3503.317397	346919.837583	49.109364
3503.445027	346912.181941	49.114369
3503.221265	346924.154675	49.119373
3503.382629	346914.584777	49.124378
3503.633312	346912.229214	49.129383
3503.315192	346910.116287	49.134388
3503.481034	346915.206211	49.139393
3503.408903	346911.883589	49.144397
3503.350775	346903.111959	49.149402
3503.412160	346921.402693	49.154407
3503.354720	346894.559812	49.159412
3503.172844	346877.128501	49.164417
3503.073723	346884.423763	49.169421
3503.434211	346877.163993	49.174426
3503.284036	346872.250211	49.179431
3503.381212	346875.416616	49.184436
3503.015460	346874.202050	49.189441
3502.909961	346881.701940	49.194445
3503.360768	346878.245739	49.199450
3503.028045	346873.029936	49.204455
3503.134205	346877.722061	49.209460
3503.403158	346869.127787	49.214465
3503.083061	346886.409844	49.219469
3503.019964	346873.184838	49.224474
3503.464612	346872.122129	49.229479
3503.302304	346874.871416	49.234484
3503.349797	346876.365822	49.239489
3503.256169	346884.169263	49.244493
3503.693451	346878.500848	49.249498
3503.147263	346880.089111	49.254503
3503.067008	346882.138212	49.259508
3503.276561	346879.025580	49.264513
3503.041053	346889.243968	49.269517
3503.514786	346883.849767	49.274522
3503.237470	346881.094081	49.279527
3503.110435	346877.703780	49.284532
3503.334421	346864.077054	49.289537
3503.344489	346857.941678	49.294541
3503.288527	346849.042435	49.299546
3503.042825	346853.891998	49.304551
3503.194167	346855.090012	49.309556
3503.285682	346846.651048	49.314561
3502.974694	346858.332158	49.319565
3503.395445	346848.695790	49.324570
3503.310335	346849.269424	49.329575
3503.527643	346855.852904	49.334580
3503.584505	346861.443656	49.339585
3503.017987	346865.453104	49.344589
3502.814538	346858.002510	49.349594
3503.320995	346861.053308	49.354599
3502.923012	346852.539017	49.359604
3503.406384	346847.677788	49.364609
3503.058992	346862.164409	49.369613
3503.408248	346861.829446	49.374618
3503.423221	346857.093173	49.379623
3503.769823	346855.104228	49.384628
3503.524892	346853.106990	49.389633
3503.396296	346828.744205	49.394637
3503.433737	346823.393520	49.399642
3503.422088	346826.195348	49.404647
3503.373302	346834.806181	49.409652
3503.549568	346808.333551	49.414657
3503.220556	346820.831993	49.419661
3503.430704	346824.387779	49.424666
3503.392994	346826.939203	49.429671
3503.242173	346812.913577	49.434676
3503.320953	346797.909912	49.439681
3502.985332	346801.501076	49.444685
3503.197932	346786.832585	49.449690
3503.193960	346792.509318	49.454695
3503.005483	346790.757677	49.459700
3503.340137	346789.839618	49.464705
3503.166089	346789.561933	49.469709
3503.602402	346787.253375	49.474714
3503.444594	346792.012690	49.479719
3503.301797	346798.627654	49.484724
3503.355069	346791.365537	49.489729
3503.341714	346801.167035	49.494733
3503.681468	346796.939363	49.499738
3503.568078	346798.102873	49.504743
3503.208691	346790.396946	49.509748
3503.341654	346767.723545	49.514753
3503.025445	346760.825264	49.519757
3503.238026	346758.170289	49.524762
3503.345801	346762.938526	49.529767
3503.363168	346755.834794	49.534772
3503.566231	346754.988443	49.539777
3503.500235	346761.922151	49.544781
3503.646487	346759.481281	49.549786
3503.741521	346755.801342	49.554791
3503.399965	346763.338566	49.559796
3503.408697	346743.459104	49.564801
3503.373328	346744.355757	49.569805
3503.303615	346740.523695	49.574810
3503.181343	346745.684635	49.579815
3503.417593	346739.335322	49.584820
3503.427177	346733.301818	49.589825
3503.496804	346746.042684	49.594829
3503.632930	346734.975055	49.599834
3503.299833	346745.463421	49.604839
3502.908347	346730.890417	49.609844
3503.191189	346736.572717	49.614849
3503.640643	346739.581628	49.619853
3503.399444	346728.777270	49.624858
3503.046752	346709.667601	49.629863
3503.027719	346707.889170	49.634868
3503.359146	346694.830823	49.639873
3503.114537	346703.701706	49.644877
3503.496366	346703.208878	49.649882
3503.351892	346694.705391	49.654887
3503.188811	346709.977390	49.659892
3503.311725	346714.514165	49.664897
3503.354537	346716.162030	49.669901
3503.489938	346706.825274	49.674906
3503.176964	346713.314437	49.679911
3503.112447	346712.332221	49.684916
3503.154968	346701.177574	49.689921
3503.123616	346718.694010	49.694925
3503.271175	346706.071972	49.699930
3503.537109	346712.775043	49.704935
3503.019238	346710.566426	49.709940
3503.363148	346710.130498	49.714945
3503.332993	346699.343675	49.719949
3503.258878	346676.321189	49.724954
3502.981212	346676.619837	49.729959
3503.228176	346674.850257	49.734964
3503.237583	346667.824131	49.739969
3502.889514	346670.093746	49.744973
3503.240541	346671.489266	49.749978
3503.043068	346678.952818	49.754983
3503.070100	346688.111640	49.759988
3502.819352	346678.530498	49.764993
3502.755155	346702.924282	49.769997
3503.283092	346706.226216	49.775002
3503.111146	346710.962321	49.780007
3503.016066	346716.551655	49.785012
3503.376283	346698.347373	49.790017
3503.404434	346718.425094	49.795021
3503.451224	346703.324652	49.800026
3503.554320	346684.906491	49.805031
3503.285086	346675.582794	49.810036
3503.072474	346668.769934	49.815041
3503.092925	346672.762958	49.820045
3503.070858	346674.319271	49.825050
3503.108158	346676.120724	49.830055
3503.074198	346678.035251	49.835060
3503.090532	346676.912990	49.840065
3503.077530	346680.504064	49.845069
3503.299267	346669.651960	49.850074
3503.529179	346682.367500	49.855079
3503.304701	346682.810454	49.860084
3503.190845	346678.374509	49.865089
3503.498160	346682.296729	49.870093
3503.570836	346680.325632	49.875098
3503.750933	346679.584720	49.880103
3503.482164	346673.340691	49.885108
3503.507634	346644.499297	49.890113
3503.118171	346651.458704	49.895117
3503.477134	346642.722904	49.900122
3503.389822	346644.111366	49.905127
3503.375292	346641.186861	49.910132
3503.189069	346641.063815	49.915137
3503.189933	346651.397592	49.920141
3503.548054	346641.414756	49.925146
3503.505091	346648.141217	49.930151
3503.204528	346645.287384	49.935156
3503.361314	346638.237955	49.940161
3502.968167	346628.704768	49.945165
3503.000659	346629.590694	49.950170
3503.341029	346645.241263	49.955175
3503.222039	346641.646057	49.960180
3503.350927	346615.053564	49.965185
3503.004659	346613.963174	49.970189
3503.259704	346614.457583	49.975194
3503.266727	346613.565864	49.980199
3503.010853	346618.060721	49.985204
3503.089702	346611.150871	49.990209
3502.844507	346623.432487	49.995213
3503.045892	346644.679111	50.000218
3503.453116	346653.014261	50.005223
3503.026277	346635.239815	50.010228
3503.056456	346630.170238	50.015233
3502.810903	346646.778818	50.020237
3503.305070	346643.850250	50.025242
3503.601509	346656.682540	50.030247
3503.376362	346640.479713	50.035252
3503.703179	346629.992776	50.040257
3503.514233	346631.473664	50.045261
3503.248856	346628.919697	50.050266
3503.233689	346623.806382	50.055271
3503.032612	346626.638167	50.060276
3503.134365	346621.608178	50.065281
3503.182341	346637.508593	50.070285
3503.214645	346630.478842	50.075290
3503.453375	346627.310678	50.080295
3502.972693	346641.920237	50.085300
3503.265149	346643.757710	50.090305
3503.335962	346641.456024	50.095309
3503.531584	346645.574071	50.100314
3503.299147	346637.262648	50.105319
3503.190986	346618.521529	50.110324
3503.244515	346601.409252	50.115329
3502.874616	346597.650090	50.120333
3503.153960	346606.107273	50.125338
3503.126158	346608.784403	50.130343
3502.880047	346621.193425	50.135348
3503.395073	346633.965712	50.140353
3503.126430	346637.622655	50.145357
3503.274205	346622.149892	50.150362
3502.909575	346608.514351	50.155367
3503.143880	346630.341183	50.160372
3503.264140	346635.743767	50.165377
3503.030826	346649.576097	50.170381
3503.333497	346635.936877	50.175386
3503.386499	346617.730233	50.180391
3503.245706	346606.171857	50.185396
3502.995979	346604.506251	50.190401
3503.123298	346613.089276	50.195405
3503.287952	346616.194124	50.200410
3503.352262	346612.391771	50.205415
3503.341865	346614.557099	50.210420
3503.561864	346616.431480	50.215425
3503.052703	346608.596492	50.220429
3503.293868	346607.413233	50.225434
3503.404019	346607.319690	50.230439
3503.092937	346606.529166	50.235444
3503.291744	346607.083370	50.240449
3503.213655	346609.004876	50.245453
3503.212470	346613.612184	50.250458
3503.280585	346625.487932	50.255463
3503.450217	346611.589762	50.260468
3503.472636	346600.616441	50.265473
3502.924508	346607.040983	50.270477
3503.637329	346598.274687	50.275482
3503.224167	346576.807456	50.280487
3502.899726	346571.030361	50.285492
3503.503284	346577.069214	50.290497
3503.225398	346580.854885	50.295501
3503.740751	346580.519114	50.300506
3503.787291	346573.996155	50.305511
3503.771790	346577.587630	50.310516
3503.834478	346569.305897	50.315521
3503.504568	346552.890535	50.320525
3503.176162	346544.288841	50.325530
3503.199437	346546.525206	50.330535
3502.949195	346547.532189	50.335540
3503.254021	346547.026082	50.340545
3503.229128	346538.987263	50.345549
3503.000806	346536.427434	50.350554
3503.448390	346548.574089	50.355559
3503.069020	346544.027395	50.360564
3503.338484	346533.396792	50.365569
3503.394013	346550.466852	50.370573
3503.210695	346543.420273	50.375578
3503.524296	346546.017980	50.380583
3503.158318	346549.563055	50.385588
3503.467301	346547.172807	50.390593
3503.193339	346546.274604	50.395597
3503.262645	346542.471457	50.400602
3503.057916	346537.591722	50.405607
3503.077483	346535.985350	50.410612
3503.400082	346531.887634	50.415617
3503.115787	346535.292533	50.420621
3503.123562	346522.539839	50.425626
3503.291301	346519.077463	50.430631
3503.117506	346524.093853	50.435636
3503.287073	346518.493179	50.440641
3503.240723	346523.413064	50.445645
3503.545614	346520.285340	50.450650
3503.326566	346515.026080	50.455655
3503.411633	346521.401433	50.460660
3503.830226	346521.971797	50.465665
3503.423640	346523.970691	50.470669
3503.100938	346522.494786	50.475674
3503.633486	346523.225302	50.480679
3503.102802	346510.786803	50.485684
3503.510728	346498.505345	50.490689
3503.637093	346496.551206	50.495693
3503.372892	346480.863557	50.500698
3503.480298	346483.035720	50.505703
3503.032850	346495.858387	50.510708
3503.309856	346488.306336	50.515713
3503.303178	346501.237487	50.520717
3503.509647	346487.028033	50.525722
3503.411224	346471.823224	50.530727
3503.359171	346455.109382	50.535732
3503.349868	346426.604258	50.540737
3503.273209	346403.022108	50.545741
3502.882825	346356.505891	50.550746
3502.970485	346309.125032	50.555751
3502.819351	346271.606587	50.560756
3502.567784	346202.720917	50.565761
3502.384637	346123.516021	50.570765
3501.644260	346043.431907	50.575770
3501.911652	345964.664619	50.580775
3501.180717	345876.586622	50.585780
3500.943995	345766.922731	50.590785
3500.532089	345674.187028	50.595789
3500.261444	345562.313713	50.600794
3500.104854	345441.615427	50.605799
3499.514659	345339.617043	50.610804
3499.040210	345212.987076	50.615809
3498.541839	345088.549584	50.620813
3498.501567	344962.537666	50.625818
3497.987684	344825.655463	50.630823
3497.718167	344687.487096	50.635828
3497.093337	344550.316350	50.640833
3496.426750	344412.719178	50.645837
3496.136282	344255.844849	50.650842
3495.568242	344107.693644	50.655847
3494.603237	343960.597517	50.660852
3494.666590	343795.520876	50.665857
3494.042938	343645.239198	50.670861
3493.316584	343472.090404	50.675866
3493.067239	343309.683595	50.680871
3492.472468	343148.450929	50.685876
3491.852364	342972.000330	50.690881
3491.245965	342804.430526	50.695885
3490.590151	342631.013610	50.700890
3490.317130	342452.775734	50.705895
3489.555927	342283.905340	50.710900
3489.028706	342104.230278	50.715905
3487.879846	341940.638369	50.720909
3487.377316	341754.467485	50.725914
3487.037710	341591.993973	50.730919
3486.134085	341408.761822	50.735924
3485.451599	341229.134193	50.740929
3484.864497	341062.651106	50.745933
3484.711704	340877.593198	50.750938
3484.025290	340693.840943	50.755943
3483.111403	340512.949618	50.760948
3482.323378	340321.728545	50.765953
3482.114954	340138.357275	50.770957
3481.307926	339957.651092	50.775962
3480.860256	339766.603614	50.780967
3479.912928	339591.646016	50.785972
3479.392923	339386.608343	50.790977
3478.798667	339205.790003	50.795981
3478.215836	339027.845832	50.800986
3477.654643	338826.580302	50.805991
3476.422560	338642.322863	50.810996
3476.082400	338451.738101	50.816001
3475.249782	338281.493569	50.821005
3474.912457	338082.837735	50.826010
3473.947114	337899.936083	50.831015
3473.302555	337708.989963	50.836020
3472.769685	337520.342143	50.841025
3472.218248	337332.714966	50.846029
3471.396293	337138.791383	50.851034
3470.725292	336937.486443	50.856039
3470.216004	336769.248820	50.861044
3469.451007	336563.451795	50.866049
3468.877670	336377.505501	50.871053
3468.036753	336187.757025	50.876058
3467.746970	335983.945072	50.881063
3466.635106	335798.031397	50.886068
3466.253068	335607.266819	50.891073
3465.163191	335424.632586	50.896077
3464.420349	335225.675895	50.901082
3464.159986	335037.207070	50.906087
3463.296552	334855.146474	50.911092
3462.354264	334667.726365	50.916097
3462.011993	334486.091532	50.921101
3461.558972	334295.716364	50.926106
3461.213653	334112.400835	50.931111
3460.168135	333914.328290	50.936116
3459.806031	333721.773271	50.941121
3458.684082	333526.664795	50.946125
3457.916034	333343.897775	50.951130
3457.182626	333140.809411	50.956135
3456.532893	332961.637708	50.961140
3456.103921	332765.755643	50.966145
3455.211184	332581.529793	50.971149
3454.588363	332391.863660	50.976154
3453.829030	332199.087244	50.981159
3452.948010	332015.418159	50.986164
3452.655672	331827.531271	50.991169
3451.829417	331640.339315	50.996173
3451.053274	331461.081997	51.001178
3450.782181	331273.801313	51.006183
3449.980613	331091.466617	51.011188
3449.301688	330884.086189	51.016193
3448.696559	330706.123824	51.021197
3448.189142	330509.993444	51.026202
3447.725247	330315.383193	51.031207
3446.677388	330131.761193	51.036212
3446.459257	329931.713778	51.041217
3445.334449	329744.284136	51.046221
3444.437445	329567.281711	51.051226
3443.854211	329363.751683	51.056231
3443.146164	329177.858657	51.061236
3442.392484	328986.091283	51.066241
3441.786018	328807.691789	51.071245
3441.091219	328616.245142	51.076250
3440.461397	328431.636352	51.081255
3439.959088	328245.479379	51.086260
3439.101599	328049.016040	51.091265
3438.536409	327863.580956	51.096269
3437.817812	327683.007040	51.101274
3437.008346	327493.867111	51.106279
3436.145693	327309.674351	51.111284
3435.934927	327116.161578	51.116289
3435.055019	326942.994843	51.121293
3434.298251	326751.578847	51.126298
3433.929403	326566.236941	51.131303
3432.954217	326391.836517	51.136308
3432.486447	326195.637888	51.141313
3431.738947	326017.941732	51.146317
3431.072317	325825.516305	51.151322
3430.522788	325644.783697	51.156327
3429.957388	325466.039111	51.161332
3429.058512	325278.817582	51.166337
3428.608449	325088.596685	51.171341
3428.120936	324896.497178	51.176346
3427.115525	324704.300888	51.181351
3426.331477	324527.192846	51.186356
3425.770095	324330.418916	51.191361
3425.396678	324149.527854	51.196365
3424.336480	323960.953946	51.201370
3423.585545	323782.871566	51.206375
3422.909926	323599.099082	51.211380
3422.158794	323411.875427	51.216385
3421.008725	323233.447620	51.221389
3420.612684	323049.044125	51.226394
3420.161931	322868.748147	51.231399
3419.329126	322693.731774	51.236404
3419.055502	322516.105945	51.241409
3418.174645	322338.270233	51.246413
3417.349712	322152.608636	51.251418
3417.154201	321971.353805	51.256423
3416.372403	321789.682074	51.261428
3415.628958	321604.744810	51.266433
3414.843947	321419.762805	51.271437
3414.178363	321244.818920	51.276442
3413.822463	321059.513688	51.281447
3412.683675	320881.766730	51.286452
3412.081386	320697.289023	51.291457
3411.522713	320523.625371	51.296461
3410.860150	320347.915389	51.301466
3410.238328	320162.166573	51.306471
3409.194882	319991.277532	51.311476
3408.989871	319808.059215	51.316481
3408.143322	319635.712491	51.321485
3407.683569	319443.927502	51.326490
3406.745120	319264.617955	51.331495
3406.117772	319085.386177	51.336500
3405.594039	318902.318307	51.341505
3405.044567	318724.219327	51.346509
3404.242397	318538.877691	51.351514
3404.188692	318360.877861	51.356519
3403.314094	318173.102553	51.361524
3402.622959	317977.735453	51.366529
3401.468064	317804.390142	51.371533
3400.843592	317622.736169	51.376538
3400.264463	317431.627983	51.381543
3398.970537	317265.407806	51.386548
3398.532388	317086.957141	51.391553
3398.096262	316909.855365	51.396557
3397.262189	316728.181934	51.401562
3396.719141	316556.800135	51.406567
3395.721396	316377.978336	51.411572
3395.045470	316199.971067	51.416577
3394.296438	316036.947383	51.421581
3394.109083	315862.325240	51.426586
3393.647595	315671.373270	51.431591
3392.818018	315501.842857	51.436596
3392.350313	315331.032695	51.441601
3391.663717	315134.564300	51.446605
3390.933020	314962.700182	51.451610
3389.989091	314785.598556	51.456615
3389.501778	314615.528739	51.461620
3388.874745	314422.105183	51.466625
3388.093643	314254.169245	51.471629
3387.312317	314065.785759	51.476634
3386.840109	313895.534130	51.481639
3386.077753	313720.642783	51.486644
3385.704606	313533.899865	51.491649
3384.727635	313360.926184	51.496653
3383.898188	313189.405796	51.501658
3383.624476	313002.620760	51.506663
3382.643532	312824.350348	51.511668
3382.101345	312640.433641	51.516673
3381.361927	312471.164171	51.521677
3380.534803	312301.831917	51.526682
3379.997949	312120.561755	51.531687
3379.363964	311950.358100	51.536692
3378.725942	311769.892752	51.541697
3378.014323	311591.934245	51.546701
3377.312781	311420.136216	51.551706
3376.763676	311249.892606	51.556711
3375.821081	311070.314620	51.561716
3375.222944	310899.390700	51.566721
3374.756798	310724.447733	51.571725
3373.859028	310551.329808	51.576730
3373.666795	310370.307904	51.581735
3372.778928	310197.951818	51.586740
3372.209973	310019.382611	51.591745
3371.477362	309844.938818	51.596749
3370.978820	309658.616680	51.601754
3370.505739	309474.047287	51.606759
3369.363844	309302.901439	51.611764
3369.211117	309121.896829	51.616769
3368.182160	308945.359540	51.621773
3367.554966	308763.079792	51.626778
3367.065315	308583.477296	51.631783
3366.254911	308402.830271	51.636788
3365.501940	308231.570469	51.641793
3364.617801	308058.701414	51.646797
3364.269023	307872.964001	51.651802
3363.291810	307694.328594	51.656807
3362.727693	307531.186784	51.661812
3362.321637	307342.147178	51.666817
3361.270634	307170.754800	51.671821
3360.911440	306991.995194	51.676826
3360.464150	306808.741922	51.681831
3359.475957	306642.381024	51.686836
3359.108877	306469.911866	51.691841
3358.275589	306284.961791	51.696845
3357.497488	306109.017476	51.701850
3357.032121	305924.823599	51.706855
3355.583883	305762.532413	51.711860
3355.272116	305579.357848	51.716865
3354.754425	305410.196174	51.721869
3353.648710	305234.862760	51.726874
3353.459754	305064.069797	51.731879
3352.550321	304896.904824	51.736884
3352.089695	304723.200389	51.741889
3351.366771	304550.657710	51.746893
3350.592814	304374.175700	51.751898
3350.195720	304198.092248	51.756903
3349.474991	304032.322470	51.761908
3348.757439	303847.885554	51.766913
3348.006957	303678.071002	51.771917
3347.214211	303487.253586	51.776922
3346.949447	303322.989752	51.781927
3346.112764	303154.028590	51.786932
3345.372075	302980.111652	51.791937
3344.711819	302809.696093	51.796941
3343.929883	302632.143629	51.801946
3344.037765	302455.748990	51.806951
3342.454109	302284.689424	51.811956
3341.915214	302105.544463	51.816961
3341.321581	301941.305643	51.821965
3340.657258	301773.308832	51.826970
3340.346432	301596.342757	51.831975
3339.235642	301421.973226	51.836980
3338.666395	301240.336364	51.841985
3337.893855	301083.255477	51.846989
3337.245751	300908.353801	51.851994
3336.447434	300728.611618	51.856999
3335.949552	300573.040232	51.862004
3335.601541	300393.226451	51.867009
3334.825665	300212.257753	51.872013
3334.027026	300043.108887	51.877018
3333.069879	299864.689653	51.882023
3332.779938	299713.439323	51.887028
3332.084404	299526.039604	51.892033
3331.200828	299357.743867	51.897037
3330.376936	299190.991984	51.902042
3329.930586	299019.112368	51.907047
3329.340342	298852.985330	51.912052
3328.826412	298680.835931	51.917057
3327.967490	298507.976926	51.922061
3327.310203	298332.590121	51.927066
3326.973079	298174.750013	51.932071
3325.944037	297995.754462	51.937076
3325.595455	297817.491511	51.942081
3324.821690	297644.134324	51.947085
3324.036586	297475.999466	51.952090
3323.682097	297308.585816	51.957095
3322.497745	297143.875426	51.962100
3321.945258	296959.022498	51.967105
3321.456107	296796.621197	51.972109
3320.616678	296619.504331	51.977114
3319.980784	296447.041029	51.982119
3319.021607	296283.211081	51.987124
3318.645073	296105.765853	51.992129
3317.868005	295943.154697	51.997133
3317.154435	295780.074956	52.002138
3316.879864	295599.939102	52.007143
3316.232853	295448.130476	52.012148
3315.529323	295266.075735	52.017153
3314.755949	295099.159362	52.022157
3313.989885	294926.842658	52.027162
3313.556251	294756.587005	52.032167
3312.922850	294601.821404	52.037172
3312.283810	294412.777695	52.042177
3311.394706	294246.159081	52.047181
3310.581862	294066.030623	52.052186
3309.979874	293904.001373	52.057191
3308.904170	293746.809318	52.062196
3308.435882	293577.449560	52.067201
3307.863806	293407.902351	52.072205
3307.119191	293242.202408	52.077210
3306.898268	293070.256402	52.082215
3305.867888	292910.560785	52.087220
3305.635796	292736.018619	52.092225
3304.812453	292567.452821	52.097229
3303.906884	292395.640073	52.102234
3303.304446	292224.899821	52.107239
3302.597618	292059.931613	52.112244
3301.846823	291896.090816	52.117249
3301.328099	291732.034928	52.122253
3300.525018	291554.857189	52.127258
3300.091954	291392.009968	52.132263
3299.398331	291224.696094	52.137268
3299.126355	291047.637728	52.142273
3298.298527	290882.789747	52.147277
3297.243243	290712.451164	52.152282
3296.934072	290538.861930	52.157287
3295.969762	290382.465014	52.162292
3295.531220	290202.758318	52.167297
3294.716014	290036.456156	52.172301
3294.174660	289868.327835	52.177306
3293.441712	289697.682945	52.182311
3292.603914	289528.480730	52.187316
3292.045357	289354.318966	52.192321
3291.455770	289197.581961	52.197325
3290.415512	289031.645885	52.202330
3289.977182	288857.948693	52.207335
3289.378140	288692.884943	52.212340
3288.801511	288527.868493	52.217345
3287.941772	288374.331797	52.222349
3287.597888	288204.897888	52.227354
3286.750110	288026.324224	52.232359
3285.831923	287862.507502	52.237364
3285.442342	287702.503668	52.242369
3284.816559	287528.249621	52.247373
3283.972025	287363.682427	52.252378
3283.744362	287191.962955	52.257383
3282.854615	287025.390780	52.262388
3282.219913	286863.413349	52.267393
3281.363105	286688.507778	52.272397
3280.665349	286518.186666	52.277402
3280.301618	286347.379680	52.282407
3279.365457	286188.836871	52.287412
3278.833581	286008.353012	52.292417
3278.322329	285845.107663	52.297421
3277.265050	285676.804072	52.302426
3276.778805	285511.568117	52.307431
3276.092111	285357.900833	52.312436
3275.280592	285186.221840	52.317441
3274.628416	285016.784227	52.322445
3274.081923	284851.557531	52.327450
3273.502763	284673.500012	52.332455
3272.253186	284522.111715	52.337460
3271.588602	284353.872801	52.342465
3271.601813	284193.116107	52.347469
3270.929591	284033.308232	52.352474
3270.056195	283862.886437	52.357479
3269.387785	283703.612676	52.362484
3268.829006	283524.303538	52.367489
3268.508899	283369.940861	52.372493
3267.398115	283204.140657	52.377498
3267.096942	283036.837043	52.382503
3265.916031	282867.762426	52.387508
3265.659839	282696.529483	52.392513
3265.147321	282522.077103	52.397517
3264.211672	282353.498358	52.402522
3263.550626	282183.118815	52.407527
3262.524718	282029.809726	52.412532
3262.183396	281856.628939	52.417537
3261.155427	281691.350012	52.422541
3260.546820	281532.830195	52.427546
3260.055988	281364.588297	52.432551
3259.214276	281200.425850	52.437556
3258.927744	281043.714149	52.442561
3258.009012	280877.908369	52.447565
3256.861052	280713.183014	52.452570
3256.746372	280554.839515	52.457575
3256.190908	280394.528248	52.462580
3255.405269	280217.215060	52.467585
3254.576040	280053.075849	52.472589
3254.005612	279897.198336	52.477594
3253.318473	279728.044791	52.482599
3252.359657	279569.529018	52.487604
3252.465208	279400.453758	52.492609
3251.850181	279237.885014	52.497613
3250.901744	279075.623671	52.502618
3250.697398	278902.700694	52.507623
3249.247947	278744.797241	52.512628
3248.772083	278582.282785	52.517633
3248.124748	278422.113053	52.522637
3247.255447	278258.336440	52.527642
3247.005083	278084.019861	52.532647
3245.990049	277931.446874	52.537652
3245.511053	277758.592653	52.542657
3245.045077	277596.229323	52.547661
3244.173182	277435.789383	52.552666
3243.330135	277270.047443	52.557671
3242.646033	277105.833914	52.562676
3242.182735	276933.766648	52.567681
3241.212584	276774.309997	52.572685
3240.725962	276614.929652	52.577690
3240.209647	276442.004813	52.582695
3239.097175	276286.085287	52.587700
3238.709719	276132.572426	52.592705
3238.260968	275973.109652	52.597709
3237.311502	275803.131236	52.602714
3236.827425	275634.887446	52.607719
3235.872284	275482.967009	52.612724
3235.333192	275314.375359	52.617729
3234.664208	275155.023814	52.622733
3234.060761	274997.088131	52.627738
3233.369323	274834.632995	52.632743
3232.456880	274674.708728	52.637748
3231.788357	274511.536856	52.642753
3231.347286	274359.993528	52.647757
3230.463328	274204.139707	52.652762
3229.786498	274042.242583	52.657767
3229.248077	273883.379776	52.662772
3228.905879	273720.512864	52.667777
3228.156642	273562.600286	52.672781
3227.326773	273403.503461	52.677786
3226.760849	273244.161142	52.682791
3225.774809	273081.905498	52.687796
3225.423490	272929.100092	52.692801
3224.653629	272763.448449	52.697805
3224.239313	272604.769842	52.702810
3223.308947	272448.821604	52.707815
3222.559119	272296.894291	52.712820
3222.263023	272138.477180	52.717825
3221.440316	271980.550897	52.722829
3220.410568	271824.796730	52.727834
3220.274512	271658.026204	52.732839
3219.325417	271497.776888	52.737844
3218.789465	271337.767852	52.742849
3218.010597	271188.977876	52.747853
3217.329168	271029.755952	52.752858
3216.897726	270856.792538	52.757863
3215.986871	270712.276726	52.762868
3215.394081	270547.157674	52.767873
3214.558727	270387.068820	52.772877
3213.840859	270237.148736	52.777882
3213.803942	270073.113371	52.782887
3212.718235	269919.176611	52.787892
3212.036274	269762.068870	52.792897
3211.672501	269599.256858	52.797901
3210.879335	269438.219192	52.802906
3210.314288	269275.158945	52.807911
3209.356380	269108.875483	52.812916
3209.148097	268953.399351	52.817921
3208.250728	268789.169320	52.822925
3207.147376	268633.096297	52.827930
3206.696913	268469.508753	52.832935
3206.100166	268315.494991	52.837940
3205.249155	268164.755963	52.842945
3204.591422	268004.359401	52.847949
3204.074341	267845.443256	52.852954
3203.489778	267692.497396	52.857959
3202.785647	267532.566737	52.862964
3202.129657	267376.474208	52.867969
3201.156457	267219.616931	52.872973
3200.537818	267068.612225	52.877978
3200.052833	266903.884533	52.882983
3199.127671	266744.116430	52.887988
3198.744775	266585.179437	52.892993
3197.979412	266438.782408	52.897997
3197.338552	266276.167981	52.903002
3197.126020	266121.508307	52.908007
3195.950294	265977.086462	52.913012
3195.431483	265825.888078	52.918017
3194.834349	265658.708161	52.923021
3193.856249	265503.074701	52.928026
3193.457596	265345.388574	52.933031
3192.471548	265189.858360	52.938036
3192.190028	265046.619688	52.943041
3191.295483	264892.781470	52.948045
3190.774045	264731.753222	52.953050
3189.964493	264570.592349	52.958055
3189.087145	264429.103595	52.963060
3188.600170	264270.616889	52.968065
3188.102274	264121.758889	52.973069
3187.258527	263965.875563	52.978074
3186.694644	263798.716635	52.983079
3186.061389	263651.102707	52.988084
3185.401856	263499.265313	52.993089
3184.576409	263350.917879	52.998093
3184.002963	263186.944249	53.003098
3183.597795	263025.974756	53.008103
3182.759769	262879.717888	53.013108
3182.368293	262723.177794	53.018113
3181.538802	262561.486158	53.023117
3180.376439	262403.336372	53.028122
3179.804760	262260.628611	53.033127
3179.052080	262114.078436	53.038132
3178.731453	261959.055575	53.043137
3178.162401	261804.199437	53.048141
3177.561273	261658.313130	53.053146
3177.051225	261491.452466	53.058151
3176.028930	261347.008212	53.063156
3175.516247	261186.667893	53.068161
3174.853839	261023.549898	53.073165
3174.134430	260876.969592	53.078170
3173.730912	260717.962051	53.083175
3172.661119	260567.515311	53.088180
3171.981233	260406.998143	53.093185
3171.382995	260252.376656	53.098189
3170.591325	260113.397560	53.103194
3169.808165	259942.658990	53.108199
3168.968130	259806.514617	53.113204
3168.596659	259655.601336	53.118209
3168.140663	259500.015471	53.123213
3167.439918	259357.304106	53.128218
3166.496616	259198.357399	53.133223
3165.990870	259046.447013	53.138228
3165.474995	258892.271706	53.143233
3164.845943	258740.355547	53.148237
3163.738539	258592.284369	53.153242
3163.713811	258435.026458	53.158247
3162.645106	258290.616662	53.163252
3161.911377	258136.909245	53.168257
3161.418919	257987.544156	53.173261
3160.851405	257829.863176	53.178266
3160.217651	257681.335596	53.183271
3159.269773	257530.667617	53.188276
3158.587320	257372.903261	53.193281
3158.122756	257226.590334	53.198285
3157.383505	257083.809996	53.203290
3156.957104	256921.828785	53.208295
3156.522218	256776.479211	53.213300
3155.643494	256621.726116	53.218305
3155.254691	256456.886951	53.223309
3153.888350	256308.756334	53.228314
3153.043812	256157.589046	53.233319
3152.601781	256010.509336	53.238324
3151.980407	255858.390125	53.243329
3151.780131	255706.713733	53.248333
3150.885834	255547.303372	53.253338
3150.347719	255391.707783	53.258343
3149.512930	255245.938648	53.263348
3148.905308	255087.476497	53.268353
3148.295471	254934.261048	53.273357
3147.537604	254790.848510	53.278362
3146.900432	254628.112919	53.283367
3145.955955	254480.629931	53.288372
3145.369065	254321.604827	53.293377
3144.690981	254178.103705	53.298381
3143.954544	254026.156874	53.303386
3143.774270	253880.055964	53.308391
3142.902590	253738.674096	53.313396
3142.062599	253576.964688	53.318401
3141.740291	253432.847551	53.323405
3140.951973	253277.140419	53.328410
3140.415270	253115.077812	53.333415
3139.318523	252968.180355	53.338420
3138.835774	252817.467696	53.343425
3138.126125	252674.049111	53.348429
3136.954421	252516.849813	53.353434
3136.747086	252371.518370	53.358439
3136.145949	252232.896187	53.363444
3135.234641	252080.571151	53.368449
3134.684959	251937.586243	53.373453
3134.076292	251784.602369	53.378458
3133.526798	251639.453004	53.383463
3132.812033	251498.175378	53.388468
3131.793059	251344.238155	53.393473
3131.649814	251186.724496	53.398477
3130.819510	251050.711645	53.403482
3130.402424	250887.358813	53.408487
3129.684217	250746.922751	53.413492
3128.666122	250600.498696	53.418497
3128.429027	250453.747446	53.423501
3127.740581	250305.972693	53.428506
3126.983233	250151.282099	53.433511
3126.048875	249997.510988	53.438516
3125.529305	249846.704886	53.443521
3124.982187	249702.422679	53.448525
3123.872612	249559.451996	53.453530
3123.318442	249411.402145	53.458535
3122.642133	249259.118885	53.463540
3122.196554	249111.943451	53.468545
3121.459463	248961.834732	53.473549
3120.610048	248815.894931	53.478554
3120.202840	248667.822524	53.483559
3119.448790	248530.220821	53.488564
3118.693728	248374.665749	53.493569
3117.884719	248227.905194	53.498573
3117.626354	248092.670193	53.503578
3116.856254	247937.907398	53.508583
3116.070130	247794.225040	53.513588
3115.483076	247645.749166	53.518593
3114.813614	247506.428784	53.523597
3114.028293	247361.549815	53.528602
3113.764456	247208.210156	53.533607
3112.779188	247067.590470	53.538612
3111.885501	246924.053312	53.543617
3111.767811	246764.349977	53.548621
3110.949053	246628.033570	53.553626
3110.468554	246472.844502	53.558631
3109.647148	246324.203336	53.563636
3109.191233	246176.421253	53.568641
3108.173239	246026.334496	53.573645
3107.424389	245877.198469	53.578650
3106.937772	245735.075103	53.583655
3105.935296	245587.914918	53.588660
3105.372979	245441.652926	53.593665
3104.810918	245295.009065	53.598669
3104.144927	245156.810923	53.603674
3103.514042	245011.960850	53.608679
3102.895965	244876.633021	53.613684
3102.189300	244721.481703	53.618689
3101.495317	244579.188632	53.623693
3100.923967	244429.669578	53.628698
3100.298236	244283.953648	53.633703
3099.263998	244147.902988	53.638708
3098.835332	243998.514631	53.643713
3098.575934	243849.201518	53.648717
3097.451764	243701.044046	53.653722
3097.139475	243550.135330	53.658727
3096.112242	243407.285100	53.663732
3095.332162	243259.684845	53.668737
3094.854643	243117.690153	53.673741
3094.047315	242979.949570	53.678746
3093.683707	242826.961681	53.683751
3092.851265	242685.787597	53.688756
3092.078724	242542.516053	53.693761
3091.550648	242399.180519	53.698765
3090.981553	242260.155232	53.703770
3090.282136	242104.191031	53.708775
3089.690561	241960.254892	53.713780
3088.744261	241801.758182	53.718785
3088.308217	241664.240406	53.723789
3087.408639	241524.249657	53.728794
3087.086763	241375.967956	53.733799
3086.020897	241243.999812	53.738804
3085.277277	241103.501035	53.743809
3084.726292	240964.117850	53.748813
3084.302407	240821.404296	53.753818
3083.230152	240675.890551	53.758823
3082.564593	240540.371166	53.763828
3082.118585	240394.096573	53.768833
3081.379142	240249.192762	53.773837
3080.405602	240127.040590	53.778842
3079.835011	239976.533649	53.783847
3079.401099	239840.239939	53.788852
3078.812773	239703.410610	53.793857
3078.221689	239563.220570	53.798861
3077.639671	239425.015493	53.803866
3077.028659	239286.738778	53.808871
3076.157540	239141.475230	53.813876
3075.633270	238986.200419	53.818881
3074.679481	238845.508452	53.823885
3073.881016	238714.035609	53.828890
3073.529870	238565.532938	53.833895
3073.021462	238426.477111	53.838900
3072.102360	238288.581417	53.843905
3071.685180	238139.555018	53.848909
3070.661006	237993.655117	53.853914
3069.929010	237853.922402	53.858919
3069.226861	237724.294367	53.863924
3068.894166	237574.262265	53.868929
3068.082811	237436.605229	53.873933
3067.247815	237298.315511	53.878938
3066.717013	237153.000713	53.883943
3066.001154	237019.657960	53.888948
3065.159154	236895.145829	53.893953
3064.840279	236761.282217	53.898957
3064.356994	236619.423702	53.903962
3063.759299	236468.620245	53.908967
3062.982547	236333.276354	53.913972
3062.355872	236185.533534	53.918977
3061.861018	236053.048246	53.923981
3061.070096	235914.676964	53.928986
3060.694906	235770.612614	53.933991
3059.906212	235620.706370	53.938996
3058.985554	235472.119868	53.944001
3058.428901	235332.719208	53.949005
3057.563716	235182.443756	53.954010
3057.219989	235044.155642	53.959015
3056.510889	234903.175502	53.964020
3055.943096	234743.584963	53.969025
3055.143851	234599.029185	53.974029
3054.221650	234466.664511	53.979034
3053.645139	234319.043754	53.984039
3052.877528	234193.835600	53.989044
3052.414802	234040.391640	53.994049
3051.618689	233903.067905	53.999053
3050.835098	233771.293331	54.004058
3050.269346	233623.111717	54.009063
3049.536831	233488.757669	54.014068
3048.798472	233351.323710	54.019073
3048.514472	233216.237008	54.024077
3047.631700	233071.976772	54.029082
3046.839664	232929.153772	54.034087
3046.277526	232797.523699	54.039092
3045.435171	232656.160448	54.044097
3044.743210	232513.831478	54.049101
3044.361331	232382.504457	54.054106
3043.942114	232235.473055	54.059111
3042.938714	232097.420805	54.064116
3042.292065	231963.768245	54.069121
3041.694925	231815.441600	54.074125
3040.885070	231694.648385	54.079130
3040.085322	231546.608858	54.084135
3039.493398	231414.909027	54.089140
3039.058673	231275.061988	54.094145
3038.323457	231142.392187	54.099149
3037.328437	231011.826149	54.104154
3036.906804	230857.184048	54.109159
3035.764103	230731.683317	54.114164
3035.199670	230589.158845	54.119169
3034.707450	230461.034764	54.124173
3034.015648	230324.845487	54.129178
3033.267664	230188.945391	54.134183
3032.561775	230047.717260	54.139188
3032.280084	229915.486691	54.144193
3031.601427	229784.541325	54.149197
3030.763888	229646.721106	54.154202
3030.120543	229510.678158	54.159207
3029.613181	229384.162099	54.164212
3028.720666	229250.476019	54.169217
3028.299237	229106.887314	54.174221
3027.447336	228978.924121	54.179226
3026.940905	228839.703266	54.184231
3026.402200	228712.938509	54.189236
3025.671827	228569.908812	54.194241
3025.145397	228428.323841	54.199245
3024.287323	228299.064072	54.204250
3023.746788	228152.465851	54.209255
3022.824828	228023.242066	54.214260
3022.258402	227888.233370	54.219265
3021.936520	227742.161383	54.224269
3020.929484	227613.664598	54.229274
3020.159744	227470.006412	54.234279
3019.644844	227335.499653	54.239284
3018.829533	227198.061692	54.244289
3018.138733	227069.923047	54.249293
3017.727724	226940.772782	54.254298
3017.201215	226791.195708	54.259303
3016.367119	226665.906542	54.264308
3015.333404	226538.943271	54.269313
3015.258925	226389.422662	54.274317
3014.616447	226259.737208	54.279322
3014.007020	226125.221878	54.284327
3013.167131	225999.947356	54.289332
3012.855955	225837.696568	54.294337
3012.035985	225704.246411	54.299341
3010.947242	225571.488265	54.304346
3010.861818	225420.965430	54.309351
3009.896868	225289.792167	54.314356
3009.265354	225147.936522	54.319361
3008.402383	225005.532169	54.324365
3007.626129	224879.409082	54.329370
3007.437436	224727.019791	54.334375
3006.331508	224599.625380	54.339380
3005.780414	224473.556396	54.344385
3005.005550	224334.041763	54.349389
3004.643236	224197.160862	54.354394
3003.911989	224058.174471	54.359399
3003.207660	223927.420449	54.364404
3002.453383	223785.013778	54.369409
3001.899292	223649.691784	54.374413
3001.019252	223511.239106	54.379418
3000.823220	223373.760444	54.384423
2999.835976	223245.700178	54.389428
2999.154347	223101.322816	54.394433
2998.688542	222957.917222	54.399437
2997.705621	222834.643410	54.404442
2997.110755	222692.022531	54.409447
2996.189870	222567.759117	54.414452
2995.367887	222432.507090	54.419457
2994.741056	222293.099933	54.424461
2994.202486	222169.502240	54.429466
2993.651375	222037.263186	54.434471
2993.291933	221909.283958	54.439476
2992.589152	221767.483845	54.444481
2991.921791	221628.568040	54.449485
2990.950388	221496.090940	54.454490
2990.650062	221366.512047	54.459495
2989.806708	221228.515912	54.464500
2989.306630	221093.749938	54.469505
2988.619331	220953.030914	54.474509
2987.503814	220824.714934	54.479514
2987.307508	220682.671189	54.484519
2986.432526	220555.565091	54.489524
2985.975668	220421.302663	54.494529
2985.243178	220289.400883	54.499533
2984.376454	220153.574443	54.504538
2983.984232	220020.651831	54.509543
2983.100334	219885.732394	54.514548
2982.493771	219745.244727	54.519553
2981.845508	219624.596341	54.524557
2981.178640	219495.078717	54.529562
2980.842863	219348.897095	54.534567
2980.097148	219216.350130	54.539572
2979.451781	219082.540047	54.544577
2978.892478	218932.041221	54.549581
2977.768225	218817.095865	54.554586
2977.351964	218679.800624	54.559591
2976.798252	218542.832905	54.564596
2975.820541	218406.276256	54.569601
2975.372190	218265.473627	54.574605
2974.591603	218133.048730	54.579610
2973.818327	218001.488500	54.584615
2973.181653	217877.175202	54.589620
2972.559320	217739.303386	54.594625
2972.336556	217600.961251	54.599629
2971.283841	217466.289445	54.604634
2970.363300	217329.865827	54.609639
2969.501000	217207.600604	54.614644
2968.973360	217077.670698	54.619649
2968.628463	216942.225931	54.624653
2967.651667	216811.922111	54.629658
2967.221236	216676.682333	54.634663
2966.408561	216545.843871	54.639668
2965.847613	216408.614115	54.644673
2965.358833	216285.158505	54.649677
2964.542180	216158.483724	54.654682
2964.177623	216024.584037	54.659687
2963.355189	215894.117484	54.664692
2962.365554	215756.320452	54.669697
2961.486731	215626.512499	54.674701
2960.918723	215498.132110	54.679706
2960.552710	215368.968993	54.684711
2960.072752	215256.676851	54.689716
2959.155659	215121.440796	54.694721
2958.596519	214974.616256	54.699725
2957.837906	214850.518605	54.704730
2957.391734	214715.947059	54.709735
2956.948320	214593.531057	54.714740
2955.946332	214457.571516	54.719745
2955.338002	214328.143262	54.724749
2954.491062	214191.561475	54.729754
2953.886806	214057.856349	54.734759
2953.182905	213935.699169	54.739764
2952.803878	213795.518355	54.744769
2952.114624	213666.880622	54.749773
2950.919976	213531.462602	54.754778
2950.446411	213402.638495	54.759783
2949.659276	213276.613584	54.764788
2949.226006	213146.408947	54.769793
2948.456254	213016.041459	54.774797
2947.495565	212897.376193	54.779802
2947.315121	212760.322721	54.784807
2946.611716	212634.960377	54.789812
2946.121645	212513.586578	54.794817
2945.636667	212384.498985	54.799821
2944.520056	212248.383945	54.804826
2944.044045	212121.421039	54.809831
2943.286133	211986.980769	54.814836
2942.772343	211861.373522	54.819841
2942.115778	211724.117601	54.824845
2941.138418	211605.037315	54.829850
2940.472035	211455.666543	54.834855
2939.978273	211343.065042	54.839860
2939.219659	211214.124939	54.844865
2938.761601	211086.372108	54.849869
2937.593195	210962.257597	54.854874
2937.150503	210831.957286	54.859879
2936.146884	210702.484261	54.864884
2935.981431	210574.151569	54.869889
2935.139155	210452.061041	54.874893
2934.467797	210328.492735	54.879898
2933.829028	210193.859195	54.884903
2933.070354	210073.232571	54.889908
2932.559296	209958.625308	54.894913
2932.382236	209815.862915	54.899917
2931.440245	209700.458879	54.904922
2930.870536	209569.226728	54.909927
2929.992801	209443.770991	54.914932
2929.468439	209299.104737	54.919937
2928.991578	209169.131476	54.924941
2927.732885	209050.711482	54.929946
2927.763781	208910.629180	54.934951
2926.791817	208789.198813	54.939956
2926.090403	208661.005824	54.944961
2925.526539	208525.982221	54.949965
2924.655529	208407.349358	54.954970
2924.153983	208274.620079	54.959975
2923.388150	208147.978361	54.964980
2922.814281	208016.202909	54.969985
2922.120310	207881.163151	54.974989
2921.098473	207766.920834	54.979994
2921.109864	207623.115519	54.984999
2920.448339	207500.467675	54.990004
2919.274626	207360.796019	54.995009
2918.923117	207231.850656	55.000013
2917.911185	207112.059030	55.005018
2917.552516	206985.177104	55.010023
2916.825673	206859.804612	55.015028
2915.942726	206731.097193	55.020033
2915.570976	206594.532984	55.025037
2914.791045	206471.753272	55.030042
2914.318978	206343.401623	55.035047
2913.619760	206219.527872	55.040052
2912.653250	206094.398571	55.045057
2912.311215	205966.828937	55.050061
2911.321509	205838.560343	55.055066
2910.612273	205708.542244	55.060071
2909.936562	205588.013220	55.065076
2909.376436	205460.631935	55.070081
2908.832532	205340.069824	55.075085
2907.798870	205216.912925	55.080090
2907.495520	205091.655307	55.085095
2907.063760	204961.925824	55.090100
2906.043287	204842.038349	55.095105
2905.457207	204705.665183	55.100109
2904.746158	204591.634320	55.105114
2904.501791	204454.876750	55.110119
2903.413902	204330.432225	55.115124
2902.626797	204199.806235	55.120129
2902.381517	204075.114308	55.125133
2901.281967	203956.437472	55.130138
2900.557044	203828.933154	55.135143
2900.127745	203704.932936	55.140148
2899.465414	203579.290024	55.145153
2898.701477	203458.804862	55.150157
2897.847268	203330.074962	55.155162
2897.550933	203207.416474	55.160167
2896.762494	203083.894439	55.165172
2896.224327	202962.890990	55.170177
2895.607430	202829.339641	55.175181
2894.561348	202707.589969	55.180186
2894.010767	202579.042771	55.185191
2893.625899	202454.936445	55.190196
2892.801214	202326.102353	55.195201
2892.122800	202196.010982	55.200205
2891.360391	202087.719940	55.205210
2890.698067	201960.884398	55.210215
2890.096434	201836.266556	55.215220
2889.532121	201709.097922	55.220225
2888.764168	201579.098524	55.225229
2887.420469	201461.394591	55.230234
2887.258041	201348.708682	55.235239
2886.407983	201236.411851	55.240244
2885.638861	201115.118108	55.245249
2885.236603	200989.783415	55.250253
2884.697076	200878.456194	55.255258
2884.183544	200747.833091	55.260263
2883.403971	200627.331066	55.265268
2882.619657	200512.136604	55.270273
2882.327750	200383.464459	55.275277
2881.430980	200282.986244	55.280282
2880.855889	200145.846157	55.285287
2880.175692	200020.443167	55.290292
2879.552782	199904.919021	55.295297
2878.623261	199778.767096	55.300301
2878.088950	199664.603773	55.305306
2877.404266	199536.606646	55.310311
2876.782966	199416.782137	55.315316
2876.213011	199303.910474	55.320321
2875.279410	199167.656779	55.325325
2874.662571	199054.271331	55.330330
2873.900171	198931.696157	55.335335
2873.188614	198813.694259	55.340340
2872.905991	198698.615100	55.345345
2872.282745	198577.380289	55.350349
2871.356933	198457.618871	55.355354
2870.925230	198330.526221	55.360359
2870.145358	198215.628646	55.365364
2869.441422	198083.604225	55.370369
2868.644737	197973.481697	55.375373
2867.867487	197861.536660	55.380378
2867.253379	197739.678799	55.385383
2866.466537	197622.823987	55.390388
2866.266586	197513.066020	55.395393
2865.731384	197389.669496	55.400397
2864.522515	197270.159194	55.405402
2864.063878	197150.021373	55.410407
2863.769808	197034.120544	55.415412
2862.991901	196913.804779	55.420417
2862.521092	196777.598482	55.425421
2861.587048	196659.751161	55.430426
2861.267567	196537.798545	55.435431
2860.425277	196408.357897	55.440436
2859.831911	196292.162553	55.445441
2859.409221	196169.056492	55.450445
2858.257973	196042.045167	55.455450
2857.856670	195914.788153	55.460455
2857.227974	195790.634042	55.465460
2856.137036	195671.439587	55.470465
2855.762721	195544.726363	55.475469
2854.717912	195438.503972	55.480474
2854.135960	195304.431399	55.485479
2853.732868	195196.224697	55.490484
2852.897452	195069.000356	55.495489
2852.346280	194947.927999	55.500493
2851.310449	194829.401168	55.505498
2850.844950	194702.170062	55.510503
2850.371317	194587.893693	55.515508
2849.482865	194478.302111	55.520513
2849.212569	194348.407099	55.525517
2848.607727	194232.739943	55.530522
2847.928997	194099.118498	55.535527
2846.927828	193983.985464	55.540532
2846.236855	193865.164531	55.545537
2845.447090	193747.924563	55.550541
2844.680885	193633.276805	55.555546
2844.289540	193511.088336	55.560551
2843.512985	193388.286808	55.565556
2842.855838	193269.703686	55.570561
2842.523088	193146.603443	55.575565
2841.572846	193024.033898	55.580570
2841.042198	192918.384311	55.585575
2840.152256	192802.994641	55.590580
2839.706295	192680.117062	55.595585
2838.874228	192563.026546	55.600589
2838.113794	192452.248571	55.605594
2837.221255	192320.116245	55.610599
2837.143922	192206.024317	55.615604
2836.204161	192091.483953	55.620609
2835.949443	191967.534540	55.625613
2834.990265	191862.972955	55.630618
2834.084535	191736.429865	55.635623
2833.551527	191623.111241	55.640628
2833.063363	191510.879983	55.645633
2832.334243	191379.067847	55.650637
2831.410041	191281.168968	55.655642
2831.176630	191165.742795	55.660647
2830.528867	191046.222034	55.665652
2829.472879	190920.862672	55.670657
2829.142161	190805.414597	55.675661
2828.536549	190690.442918	55.680666
2827.943466	190563.395341	55.685671
2827.166386	190448.451395	55.690676
2826.260637	190328.298947	55.695681
2825.749988	190209.394693	55.700685
2824.535896	190099.012001	55.705690
2824.488794	189975.530995	55.710695
2823.842863	189867.094523	55.715700
2823.002031	189747.760237	55.720705
2822.637759	189626.709534	55.725709
2821.879848	189507.871629	55.730714
2821.222523	189390.366703	55.735719
2820.354822	189270.986978	55.740724
2819.574851	189164.888868	55.745729
2819.345537	189041.413693	55.750733
2818.331418	188917.388832	55.755738
2817.526187	188801.270112	55.760743
2817.255114	188679.583658	55.765748
2816.151165	188571.222685	55.770753
2815.550342	188444.703610	55.775757
2814.948604	188330.869317	55.780762
2814.340590	188213.372232	55.785767
2813.590623	188108.302268	55.790772
2813.022192	187986.054027	55.795777
2812.876980	187874.464012	55.800781
2811.857232	187764.068721	55.805786
2811.111907	187646.340362	55.810791
2810.442924	187522.747976	55.815796
2809.670798	187404.859084	55.820801
2809.273367	187293.335850	55.825805
2808.323130	187175.539360	55.830810
2807.730912	187050.473027	55.835815
2806.917866	186946.929608	55.840820
2806.177953	186832.968196	55.845825
2805.868470	186707.412740	55.850829
2805.024594	186605.427059	55.855834
2804.638876	186482.454133	55.860839
2803.591208	186359.255605	55.865844
2802.913046	186254.025811	55.870849
2802.382093	186145.338039	55.875853
2801.735491	186029.315621	55.880858
2800.987763	185910.930537	55.885863
2800.311459	185806.044968	55.890868
2799.770135	185694.268521	55.895873
2799.351892	185567.906499	55.900877
2798.700626	185454.583283	55.905882
2798.116872	185345.625903	55.910887
2797.358571	185215.693051	55.915892
2796.690236	185104.408871	55.920897
2796.354701	184983.238502	55.925901
2795.315600	184869.749188	55.930906
2794.834497	184738.908740	55.935911
2793.890746	184624.628931	55.940916
2793.217342	184509.136226	55.945921
2792.421852	184391.055271	55.950925
2791.825309	184286.465906	55.955930
2791.283140	184165.991973	55.960935
2790.718750	184047.824435	55.965940
2789.894478	183925.703900	55.970945
2789.643118	183806.253461	55.975949
2788.562221	183687.799767	55.980954
2787.774220	183579.120721	55.985959
2787.155123	183457.299723	55.990964
2786.370082	183351.050498	55.995969
2786.054708	183237.018183	56.000973
2785.269362	183113.049163	56.005978
2784.567830	183003.238383	56.010983
2784.114037	182882.524950	56.015988
2783.482876	182768.976370	56.020993
2782.826596	182651.463147	56.025997
2781.982794	182548.977817	56.031002
2781.216608	182419.855766	56.036007
2780.697990	182300.782458	56.041012
2779.899189	182192.235743	56.046017
2779.254737	182071.885471	56.051021
2778.332367	181961.145499	56.056026
2777.828405	181846.230767	56.061031
2777.356920	181746.092547	56.066036
2776.606444	181627.083237	56.071041
2776.127054	181502.548760	56.076045
2775.149870	181392.098768	56.081050
2774.873134	181278.536079	56.086055
2774.449504	181154.833318	56.091060
2773.377882	181045.734813	56.096065
2773.063901	180929.024276	56.101069
2771.996183	180815.282797	56.106074
2771.265694	180691.757168	56.111079
2770.991744	180579.633266	56.116084
2770.365370	180459.564446	56.121089
2770.060585	180337.715076	56.126093
2768.980439	180224.028009	56.131098
2768.198259	180108.602270	56.136103
2767.633283	179988.982965	56.141108
2767.066899	179871.501189	56.146113
2766.210156	179744.881866	56.151117
2765.420602	179623.721872	56.156122
2764.968891	179513.142594	56.161127
2764.365402	179397.334315	56.166132
2763.568613	179282.765358	56.171137
2763.091544	179167.967990	56.176141
2762.160967	179044.758647	56.181146
2761.684638	178927.595927	56.186151
2761.122274	178805.321100	56.191156
2760.093391	178684.952160	56.196161
2759.873035	178563.794073	56.201165
2758.824597	178454.253332	56.206170
2758.213634	178336.019689	56.211175
2757.416754	178222.903656	56.216180
2756.828990	178099.006796	56.221185
2756.254622	177979.903431	56.226189
2755.537457	177873.338974	56.231194
2755.219834	177753.445135	56.236199
2754.549450	177636.214993	56.241204
2753.731082	177528.726209	56.246209
2753.165470	177400.770433	56.251213
2752.116833	177279.073132	56.256218
2751.551388	177159.029467	56.261223
2751.029323	177044.753799	56.266228
2750.207620	176932.319312	56.271233
2749.600013	176806.559715	56.276237
2748.518545	176705.805005	56.281242
2748.143469	176581.433799	56.286247
2747.926291	176469.299104	56.291252
2746.975627	176356.632230	56.296257
2746.471671	176238.781881	56.301261
2745.460987	176121.749833	56.306266
2744.790984	176008.416228	56.311271
2744.059794	175898.119716	56.316276
2743.288204	175787.588243	56.321281
2743.060832	175655.170861	56.326285
2742.192687	175547.338994	56.331290
2741.775254	175436.383525	56.336295
2741.032254	175319.553024	56.341300
2740.274979	175208.054231	56.346305
2739.700591	175084.087974	56.351309
2738.597112	174984.205849	56.356314
2737.964095	174856.904588	56.361319
2737.504139	174744.558701	56.366324
2736.674127	174640.462436	56.371329
2736.284682	174529.772094	56.376333
2735.498807	174415.876224	56.381338
2734.887813	174307.905166	56.386343
2734.338356	174191.352496	56.391348
2733.694995	174080.385649	56.396353
2733.105035	173958.116839	56.401357
2732.103816	173849.483883	56.406362
2731.528792	173732.186218	56.411367
2730.869342	173622.418692	56.416372
2730.135268	173512.230873	56.421377
2730.017954	173387.421616	56.426381
2729.060658	173281.250549	56.431386
2728.385646	173167.493272	56.436391
2728.013868	173055.786749	56.441396
2727.281391	172937.562507	56.446401
2726.315864	172823.203619	56.451405
2725.681483	172708.729014	56.456410
2724.892572	172598.908504	56.461415
2724.254541	172484.333382	56.466420
2723.722590	172372.056416	56.471425
2723.351062	172249.961719	56.476429
2722.351088	172142.070849	56.481434
2721.913391	172028.698924	56.486439
2721.457459	171910.980793	56.491444
2720.478395	171788.360601	56.496449
2719.998796	171668.891920	56.501453
2719.176788	171557.235508	56.506458
2718.417091	171430.804587	56.511463
2717.998438	171326.219423	56.516468
2717.085146	171221.229635	56.521473
2716.453868	171098.365744	56.526477
2715.725978	170982.702816	56.531482
2715.087679	170876.131599	56.536487
2714.345258	170768.076534	56.541492
2713.953935	170645.303227	56.546497
2713.455406	170525.090720	56.551501
2712.219950	170422.392336	56.556506
2711.982931	170309.718470	56.561511
2711.912368	170183.080684	56.566516
2710.397772	170072.008770	56.571521
2710.213312	169948.670779	56.576525
2709.381780	169836.499411	56.581530
2708.558332	169708.952373	56.586535
2708.260954	169589.944438	56.591540
2707.200305	169470.727148	56.596545
2706.698097	169352.998639	56.601549
2705.768386	169246.681536	56.606554
2705.555207	169124.240900	56.611559
2704.855718	169012.038299	56.616564
2704.226034	168894.382257	56.621569
2703.484515	168771.899278	56.626573
2702.680432	168660.210224	56.631578
2702.194764	168543.155557	56.636583
2701.864173	168414.313959	56.641588
2700.799286	168305.363148	56.646593
2700.572824	168170.465579	56.651597
2699.631060	168058.660219	56.656602
2699.092281	167931.824267	56.661607
2698.280564	167817.328593	56.666612
2697.244771	167697.566103	56.671617
2696.631954	167566.953668	56.676621
2696.134485	167457.788239	56.681626
2695.566091	167341.996559	56.686631
2694.748940	167225.112914	56.691636
2693.902993	167106.733703	56.696641
2693.406682	166984.548262	56.701645
2692.545816	166879.384030	56.706650
2692.184800	166754.062498	56.711655
2691.780944	166642.875488	56.716660
2690.766185	166530.819187	56.721665
2690.150226	166411.286741	56.726669
2689.467071	166297.665425	56.731674
2688.712306	166173.450905	56.736679
2687.917369	166055.575561	56.741684
2687.540831	165945.645145	56.746689
2687.222786	165816.670560	56.751693
2686.291063	165712.372781	56.756698
2685.613419	165599.210481	56.761703
2685.015603	165474.795409	56.766708
2684.271072	165358.936045	56.771713
2683.904712	165236.112679	56.776717
2683.043494	165109.019473	56.781722
2682.167695	164997.759558	56.786727
2681.866626	164875.054199	56.791732
2681.059220	164761.724288	56.796737
2680.367957	164635.394131	56.801741
2679.714004	164520.235097	56.806746
2679.001342	164393.120824	56.811751
2678.480363	164267.667724	56.816756
2677.473296	164152.896377	56.821761
2676.849382	164035.496263	56.826765
2676.444348	163925.550941	56.831770
2675.942535	163803.669287	56.836775
2675.314984	163684.897667	56.841780
2674.433762	163568.150132	56.846785
2674.002568	163438.311758	56.851789
2673.260501	163320.703795	56.856794
2672.589010	163202.093287	56.861799
2672.123288	163069.426326	56.866804
2671.093366	162954.891235	56.871809
2670.509150	162833.801473	56.876813
2669.847998	162710.829843	56.881818
2669.294809	162579.716987	56.886823
2668.817676	162468.121898	56.891828
2667.907855	162347.771928	56.896833
2667.660138	162216.370420	56.901837
2666.710530	162101.164167	56.906842
2666.059307	161977.595890	56.911847
2665.688931	161844.028324	56.916852
2664.498194	161721.919539	56.921857
2663.797821	161589.485906	56.926861
2662.873159	161481.651874	56.931866
2662.336873	161358.194662	56.936871
2661.859200	161235.554999	56.941876
2661.190490	161124.108864	56.946881
2660.700323	160992.203552	56.951885
2659.880175	160880.845741	56.956890
2659.191648	160753.066605	56.961895
2658.601447	160632.989605	56.966900
2657.938033	160517.933819	56.971905
2657.194937	160389.503523	56.976909
2656.506116	160288.513840	56.981914
2655.891776	160158.029800	56.986919
2655.530340	160042.304747	56.991924
2654.527965	159926.351071	56.996929
2654.041491	159795.161581	57.001933
2653.340305	159675.334257	57.006938
2652.388945	159555.432558	57.011943
2651.986155	159435.329932	57.016948
2651.311828	159309.918442	57.021953
2650.831600	159188.087209	57.026957
2650.209115	159063.723584	57.031962
2649.439829	158944.341792	57.036967
2649.017622	158823.595964	57.041972
2647.860692	158709.412493	57.046977
2647.423492	158580.686069	57.051981
2646.888528	158460.976403	57.056986
2645.923811	158343.216753	57.061991
2645.399058	158212.433353	57.066996
2644.836708	158087.860269	57.072001
2644.158550	157965.810404	57.077005
2643.414904	157848.996288	57.082010
2642.854187	157725.098024	57.087015
2642.055588	157605.712754	57.092020
2641.284522	157489.107600	57.097025
2640.777429	157356.036357	57.102029
2639.939758	157244.489476	57.107034
2639.334871	157121.121589	57.112039
2638.819889	157006.282665	57.117044
2638.270100	156887.165557	57.122049
2637.546024	156758.300671	57.127053
2636.868010	156632.962993	57.132058
2636.439363	156512.022843	57.137063
2635.984521	156385.659150	57.142068
2635.070991	156260.652531	57.147073
2634.802558	156130.688122	57.152077
2633.938068	156005.954331	57.157082
2633.088962	155881.104150	57.162087
2632.507633	155754.050960	57.167092
2631.819593	155617.633742	57.172097
2631.534617	155485.805756	57.177101
2630.437838	155365.318752	57.182106
2629.566905	155242.876911	57.187111
2629.101829	155113.265336	57.192116
2628.186826	155000.593976	57.197121
2627.945287	154863.117530	57.202125
2627.059299	154737.196910	57.207130
2626.414642	154610.908020	57.212135
2625.997781	154479.689577	57.217140
2624.942534	154364.017225	57.222145
2624.543656	154228.741953	57.227149
2623.782325	154103.198004	57.232154
2623.497554	153973.600370	57.237159
2622.568186	153839.529317	57.242164
2621.338358	153724.026658	57.247169
2621.176537	153597.360000	57.252173
2620.413075	153470.064618	57.257178
2620.072759	153348.206570	57.262183
2619.327130	153218.964524	57.267188
2618.470029	153094.481840	57.272193
2618.114526	152963.691781	57.277197
2617.559173	152833.734689	57.282202
2616.814976	152697.961045	57.287207
2616.069544	152564.692175	57.292212
2615.455534	152446.566922	57.297217
2614.804942	152311.199483	57.302221
2613.863409	152174.988954	57.307226
2613.253860	152051.373411	57.312231
2612.611786	151924.420614	57.317236
2611.905096	151799.524933	57.322241
2611.635228	151660.553605	57.327245
2610.426113	151545.156934	57.332250
2609.726533	151409.508617	57.337255
2609.602926	151281.357634	57.342260
2608.558965	151160.076705	57.347265
2608.101690	151030.683128	57.352269
2607.434504	150913.003946	57.357274
2606.888766	150776.075566	57.362279
2606.145411	150649.779249	57.367284
2605.149765	150517.981842	57.372289
2604.796558	150388.167596	57.377293
2604.038052	150253.524784	57.382298
2603.500581	150131.659021	57.387303
2602.961334	150001.837666	57.392308
2602.334244	149880.457308	57.397313
2601.832876	149731.464743	57.402317
2600.821360	149606.854518	57.407322
2600.134116	149472.648489	57.412327
2599.620218	149341.402287	57.417332
2598.633974	149214.234955	57.422337
2598.012031	149080.706518	57.427341
2597.127391	148963.729747	57.432346
2596.717176	148830.130668	57.437351
2596.315619	148709.723006	57.442356
2595.567973	148574.996494	57.447361
2594.644791	148447.542595	57.452365
2594.208237	148326.303109	57.457370
2593.618694	148206.359233	57.462375
2593.383255	148002.772468	57.467380
2591.975599	147869.017725	57.472385
2591.996402	147728.809823	57.477389
2591.169310	147603.631661	57.482394
2590.283609	147472.680777	57.487399
2589.622955	147335.238731	57.492404
2588.609449	147210.040823	57.497409
2588.064734	147072.327367	57.502413
2587.590569	146939.216542	57.507418
2586.967194	146814.212545	57.512423
2586.116567	146686.538147	57.517428
2585.231432	146564.181856	57.522433
2584.847048	146439.116051	57.527437
2584.314260	146315.929675	57.532442
2583.596106	146183.610485	57.537447
2583.298967	146054.135317	57.542452
2582.532396	145930.047087	57.547457
2582.243345	145781.433254	57.552461
2581.020691	145653.796578	57.557466
2580.570117	145520.687999	57.562471
2580.111034	145377.300599	57.567476
2579.000302	145254.858072	57.572481
2578.769387	145107.737750	57.577485
2577.906954	144976.120031	57.582490
2577.289778	144842.430763	57.587495
2576.651275	144710.372032	57.592500
2575.696258	144577.512607	57.597505
2575.289801	144446.485662	57.602509
2574.384137	144317.152234	57.607514
2573.831086	144174.013991	57.612519
2573.432112	144034.791284	57.617524
2572.326079	143910.332827	57.622529
2571.976261	143775.551069	57.627533
2570.904025	143656.895511	57.632538
2570.633745	143507.450863	57.637543
2569.938205	143384.835548	57.642548
2569.220331	143242.833253	57.647553
2568.614755	143104.791113	57.652557
2568.033660	142981.015637	57.657562
2567.367228	142839.998191	57.662567
2566.708100	142712.970485	57.667572
2565.858382	142580.382514	57.672577
2565.511537	142437.372130	57.677581
2564.532448	142299.164085	57.682586
2563.929236	142171.354655	57.687591
2563.179982	142040.633683	57.692596
2562.605133	141915.578157	57.697601
2561.908451	141769.716543	57.702605
2560.949606	141650.351926	57.707610
2560.483909	141514.607357	57.712615
2559.700761	141367.643214	57.717620
2558.958651	141252.438891	57.722625
2558.670050	141112.017567	57.727629
2558.216103	140980.403037	57.732634
2557.045075	140859.448772	57.737639
2556.788071	140719.380031	57.742644
2556.028914	140588.704997	57.747649
2555.497330	140448.871614	57.752653
2554.520991	140321.650046	57.757658
2554.241292	140185.920074	57.762663
2553.680393	140049.815989	57.767668
2552.645295	139912.707688	57.772673
2552.254665	139784.760283	57.777677
2551.658797	139638.410158	57.782682
2550.926647	139512.576341	57.787687
2550.358402	139370.720900	57.792692
2549.422312	139250.205978	57.797697
2549.172509	139101.135498	57.802701
2548.312671	138962.784059	57.807706
2547.869494	138823.058589	57.812711
2547.465120	138663.990366	57.817716
2546.127804	138551.571518	57.822721
2545.367750	138399.193150	57.827725
2544.662811	138268.506942	57.832730
2544.118438	138124.341341	57.837735
2543.469497	137998.360978	57.842740
2542.982445	137863.779741	57.847745
2542.116574	137718.358472	57.852749
2541.244174	137590.979622	57.857754
2540.785076	137454.756910	57.862759
2540.502087	137324.071524	57.867764
2539.504371	137185.597776	57.872769
2538.898591	137047.481810	57.877773
2538.311316	136917.646834	57.882778
2538.194870	136778.819356	57.887783
2537.398025	136635.933361	57.892788
2536.549540	136492.408332	57.897793
2536.018346	136351.501594	57.902797
2535.206622	136206.765244	57.907802
2534.157535	136066.678796	57.912807
2534.039162	135918.886646	57.917812
2532.973471	135798.965333	57.922817
2532.195477	135650.110327	57.927821
2531.668432	135521.732944	57.932826
2530.906961	135373.524627	57.937831
2530.426336	135246.195514	57.942836
2530.081855	135102.292559	57.947841
2529.741333	134954.896212	57.952845
2528.164394	134818.926465	57.957850
2527.767317	134678.972032	57.962855
2527.378061	134539.690315	57.967860
2526.389715	134400.961540	57.972865
2526.002891	134263.637079	57.977869
2525.264207	134117.273556	57.982874
2524.804083	133977.700907	57.987879
2524.021401	133836.033241	57.992884
2523.105785	133697.334440	57.997889
2522.478143	133553.661926	58.002893
2521.913581	133417.716185	58.007898
2520.990520	133269.036175	58.012903
2520.552940	133134.773828	58.017908
2519.956350	133007.930283	58.022913
2519.388731	132854.724742	58.027917
2518.457291	132720.021811	58.032922
2518.007563	132566.621296	58.037927
2517.218513	132435.923833	58.042932
2516.311201	132301.625536	58.047937
2516.148711	132152.487834	58.052941
2515.501723	132023.789419	58.057946
2514.798693	131877.342798	58.062951
2514.250113	131732.892093	58.067956
2513.523853	131595.989909	58.072961
2512.698612	131445.055662	58.077965
2511.619275	131313.545649	58.082970
2511.094279	131162.806659	58.087975
2510.546815	131024.202262	58.092980
2509.821892	130907.219651	58.097985
2509.757892	130749.093595	58.102989
2509.057048	130608.153042	58.107994
2507.842380	130474.547229	58.112999
2507.456737	130329.277692	58.118004
2506.942855	130189.897294	58.123009
2506.142961	130038.814158	58.128013
2505.650385	129904.093206	58.133018
2504.747334	129757.841734	58.138023
2504.102178	129610.191125	58.143028
2503.258026	129474.867509	58.148033
2503.074323	129328.491568	58.153037
2501.933921	129181.975913	58.158042
2501.284271	129050.548132	58.163047
2500.734083	128900.498463	58.168052
2500.349725	128761.460297	58.173057
2499.556637	128626.424836	58.178061
2498.864905	128485.544367	58.183066
2497.895757	128348.760075	58.188071
2497.643991	128197.244446	58.193076
2497.085075	128067.331010	58.198081
2496.393818	127910.107906	58.203085
2495.708019	127768.404628	58.208090
2495.083007	127633.499785	58.213095
2494.293269	127479.673018	58.218100
2493.698622	127343.837669	58.223105
2493.187597	127189.587344	58.228109
2492.181677	127047.252722	58.233114
2491.369969	126904.837257	58.238119
2490.648904	126765.291033	58.243124
2489.965495	126631.911655	58.248129
2489.639426	126476.594646	58.253133
2489.001446	126346.993977	58.258138
2488.194896	126203.057392	58.263143
2487.977413	126058.469415	58.268148
2486.909553	125923.681293	58.273153
2486.395206	125768.880739	58.278157
2485.508707	125625.315466	58.283162
2484.781593	125476.214209	58.288167
2484.205423	125341.249448	58.293172
2483.638978	125193.432296	58.298177
2483.056230	125043.408898	58.303181
2482.270228	124910.333609	58.308186
2481.552283	124761.768192	58.313191
2481.269226	124612.042557	58.318196
2480.147919	124476.343100	58.323201
2479.733616	124336.481365	58.328205
2478.871644	124192.754733	58.333210
2478.174338	124053.002825	58.338215
2477.742876	123912.866644	58.343220
2477.063133	123772.173723	58.348225
2476.486850	123627.427052	58.353229
2475.498115	123484.930653	58.358234
2474.770917	123347.320482	58.363239
2474.720360	123203.940367	58.368244
2473.810454	123066.563774	58.373249
2472.938069	122918.655251	58.378253
2472.595931	122775.882370	58.383258
2471.877091	122626.262299	58.388263
2471.437316	122473.729120	58.393268
2470.697772	122331.085109	58.398273
2470.063959	122192.831209	58.403277
2469.670859	122045.308687	58.408282
2468.678698	121888.066730	58.413287
2468.195013	121743.887007	58.418292
2467.207161	121603.914654	58.423297
2466.512426	121456.620992	58.428301
2465.674953	121319.102295	58.433306
2465.269691	121172.513472	58.438311
2464.456572	121028.770793	58.443316
2463.943734	120879.356493	58.448321
2463.282578	120730.652191	58.453325
2462.765801	120585.963469	58.458330
2461.906114	120438.968285	58.463335
2461.210912	120285.548668	58.468340
2460.738269	120144.715209	58.473345
2460.288566	119987.271652	58.478349
2459.394803	119844.379878	58.483354
2458.669144	119695.209208	58.488359
2458.155088	119547.681777	58.493364
2457.448757	119415.541913	58.498369
2456.635849	119262.178706	58.503373
2455.965352	119112.050409	58.508378
2455.227520	118961.959045	58.513383
2455.058636	118811.435563	58.518388
2453.839833	118674.289581	58.523393
2453.644985	118522.438811	58.528397
2452.981163	118369.108031	58.533402
2451.879278	118222.531933	58.538407
2451.578400	118064.905029	58.543412
2450.701150	117932.133295	58.548417
2450.259877	117780.129165	58.553421
2449.720377	117631.797804	58.558426
2448.761890	117476.976533	58.563431
2448.094956	117323.398553	58.568436
2447.274128	117187.143194	58.573441
2446.924542	117037.642579	58.578445
2446.210265	116893.246962	58.583450
2445.232665	116754.289303	58.588455
2444.930774	116603.234863	58.593460
2444.149929	116456.484648	58.598465
2443.514749	116308.017422	58.603469
2442.806847	116149.616240	58.608474
2442.379958	116005.275290	58.613479
2442.044002	115855.170080	58.618484
2441.024059	115718.484416	58.623489
2440.415649	115551.381766	58.628493
2439.709544	115407.805705	58.633498
2439.000706	115248.356647	58.638503
2438.726400	115091.822850	58.643508
2437.708580	114948.209948	58.648513
2437.107357	114790.892022	58.653517
2436.690143	114649.445149	58.658522
2435.683691	114489.261025	58.663527
2434.882130	114340.838028	58.668532
2434.072387	114192.309304	58.673537
2433.731276	114048.181696	58.678541
2433.311788	113894.559805	58.683546
2432.299184	113749.372547	58.688551
2431.708637	113592.815673	58.693556
2430.975727	113437.386670	58.698561
2430.854338	113284.419389	58.703565
2429.893807	113143.568500	58.708570
2429.316482	112990.770493	58.713575
2428.941705	112832.616555	58.718580
2427.876331	112677.359217	58.723585
2427.304735	112520.901241	58.728589
2426.447959	112366.145875	58.733594
2425.876295	112219.812356	58.738599
2425.423247	112060.787226	58.743604
2424.280364	111917.922300	58.748609
2423.865396	111759.388075	58.753613
2423.386786	111609.705256	58.758618
2422.510251	111451.779255	58.763623
2422.291876	111293.775303	58.768628
2421.141556	111149.088299	58.773633
2420.591762	110995.308196	58.778637
2419.967882	110848.692782	58.783642
2418.967098	110688.900235	58.788647
2418.422720	110534.436778	58.793652
2417.692743	110391.585021	58.798657
2417.443571	110240.852428	58.803661
2416.525130	110092.695398	58.808666
2415.688151	109938.719935	58.813671
2415.293258	109784.224800	58.818676
2414.392310	109628.979579	58.823681
2413.553422	109486.677052	58.828685
2413.376726	109342.493585	58.833690
2412.371449	109189.596548	58.838695
2412.023356	109031.767297	58.843700
2411.389259	108887.570194	58.848705
2410.756438	108734.566195	58.853709
2410.013617	108578.725142	58.858714
2409.049033	108431.143903	58.863719
2408.749981	108272.207695	58.868724
2407.950258	108127.546416	58.873729
2407.272809	107967.758466	58.878733
2406.857093	107813.590037	58.883738
2405.944937	107677.305972	58.888743
2405.318555	107513.965942	58.893748
2404.705932	107364.812554	58.898753
2403.950611	107207.332565	58.903757
2403.187996	107063.414143	58.908762
2402.423898	106907.365143	58.913767
2402.158896	106756.288624	58.918772
2401.017698	106611.214692	58.923777
2400.854049	106462.941099	58.928781
2400.148191	106316.867223	58.933786
2399.407202	106163.363677	58.938791
2398.808272	106003.519192	58.943796
2397.880912	105845.961192	58.948801
2397.482057	105695.699316	58.953805
2396.908386	105556.391601	58.958810
2396.270234	105390.326977	58.963815
2395.916932	105239.851373	58.968820
2394.798117	105080.971036	58.973825
2394.089771	104925.592284	58.978829
2393.620787	104775.290222	58.983834
2392.723811	104622.417693	58.988839
2392.051129	104468.057726	58.993844
2391.465898	104318.163994	58.998849
2390.738480	104161.695693	59.003853
2389.818653	104013.462043	59.008858
2389.281748	103866.037765	59.013863
2389.051800	103700.681534	59.018868
2388.016387	103556.243854	59.023873
2387.587626	103405.074960	59.028877
2387.239431	103250.037083	59.033882
2386.266967	103092.796332	59.038887
2385.615075	102933.888096	59.043892
2384.990873	102781.808939	59.048897
2384.610401	102636.289753	59.053901
2383.504624	102472.203874	59.058906
2382.605842	102313.434138	59.063911
2382.443111	102160.074179	59.068916
2381.601299	102021.933608	59.073921
2380.568636	101867.178321	59.078925
2380.160505	101714.190063	59.083930
2379.508142	101558.551851	59.088935
2378.863277	101400.312635	59.093940
2378.330724	101258.885996	59.098945
2377.931475	101086.825536	59.103949
2377.174051	100948.443235	59.108954
2376.555823	100782.382562	59.113959
2376.105664	100625.564032	59.118964
2374.955289	100478.524759	59.123969
2374.360305	100314.785391	59.128973
2373.901887	100160.489585	59.133978
2373.159973	100006.150953	59.138983
2372.399825	99849.431231	59.143988
2371.586197	99694.338536	59.148993
2370.910773	99534.949765	59.153997
2370.274805	99385.818798	59.159002
2369.605829	99234.182222	59.164007
2368.832134	99084.269492	59.169012
2368.139132	98939.660267	59.174017
2367.584977	98774.143013	59.179021
2367.073196	98628.213079	59.184026
2366.257523	98478.152392	59.189031
2365.567323	98313.065971	59.194036
2365.087166	98170.508251	59.199041
2364.481599	98016.009134	59.204045
2363.654447	97857.734311	59.209050
2362.727448	97717.571648	59.214055
2362.336488	97554.307964	59.219060
2361.831032	97405.086740	59.224065
2360.778261	97247.302243	59.229069
2360.207548	97106.306733	59.234074
2359.582671	96951.094865	59.239079
2359.117797	96793.550100	59.244084
2358.133108	96658.946255	59.249089
2357.645083	96497.100841	59.254093
2357.443050	96344.597611	59.259098
2356.775740	96198.682526	59.264103
2356.310932	96039.183283	59.269108
2355.708697	95882.212052	59.274113
2355.005496	95713.791638	59.279117
2354.229748	95547.762205	59.284122
2353.352268	95390.831697	59.289127
2352.675129	95232.963633	59.294132
2351.754143	95082.574264	59.299137
2351.532978	94914.692204	59.304141
2350.756911	94759.811087	59.309146
2349.522032	94604.895984	59.314151
2349.128396	94444.515263	59.319156
2348.710182	94292.618263	59.324161
2348.167374	94131.946355	59.329165
2347.262546	93979.012538	59.334170
2346.587171	93822.904373	59.339175
2346.247525	93666.388946	59.344180
2345.219807	93522.127408	59.349185
2344.913362	93360.326520	59.354189
2344.149424	93194.014622	59.359194
2343.597393	93037.974835	59.364199
2343.000013	92880.630712	59.369204
2342.006359	92721.061397	59.374209
2341.680215	92560.366469	59.379213
2340.746910	92398.145680	59.384218
2340.242922	92237.481294	59.389223
2339.670254	92075.231049	59.394228
2338.604133	91936.109395	59.399233
2338.430252	91768.528880	59.404237
2337.802051	91604.166718	59.409242
2336.724269	91444.607276	59.414247
2336.307656	91283.485784	59.419252
2335.257692	91126.181533	59.424257
2335.004876	90968.815408	59.429261
2334.186976	90805.605240	59.434266
2333.224843	90652.151867	59.439271
2332.765867	90490.852689	59.444276
2332.082674	90337.350947	59.449281
2331.510444	90172.629215	59.454285
2331.035903	90022.425300	59.459290
2329.965738	89857.670775	59.464295
2329.324697	89700.337282	59.469300
2328.725795	89554.797370	59.474305
2327.970859	89393.768788	59.479309
2327.377759	89245.700296	59.484314
2326.744347	89084.331386	59.489319
2326.610248	88909.646523	59.494324
2325.665497	88771.210462	59.499329
2324.994897	88608.697106	59.504333
2324.310242	88446.231575	59.509338
2323.674598	88285.147916	59.514343
2323.141983	88121.728754	59.519348
2322.426196	87977.073825	59.524353
2321.615797	87801.389345	59.529357
2320.999526	87645.353781	59.534362
2320.122243	87491.642996	59.539367
2319.833573	87321.160585	59.544372
2319.193771	87172.042298	59.549377
2318.473953	86996.033043	59.554381
2317.436462	86839.455190	59.559386
2316.924967	86680.335391	59.564391
2316.478771	86519.786408	59.569396
2315.392572	86369.533675	59.574401
2314.844655	86201.237598	59.579405
2314.281543	86049.718722	59.584410
2313.456110	85898.153771	59.589415
2312.975153	85736.544861	59.594420
2312.188634	85584.158225	59.599425
2311.631801	85416.896664	59.604429
2311.052695	85267.762997	59.609434
2310.673025	85108.329723	59.614439
2310.240506	84940.849341	59.619444
2309.440176	84787.545124	59.624449
2308.764128	84612.188784	59.629453
2308.185128	84452.918812	59.634458
2306.836234	84295.198329	59.639463
2306.625437	84126.161596	59.644468
2305.786037	83968.971252	59.649473
2305.191499	83809.518427	59.654477
2304.258940	83644.751730	59.659482
2303.672475	83488.703802	59.664487
2303.539573	83326.024887	59.669492
2302.392426	83166.436376	59.674497
2301.790782	83000.906003	59.679501
2301.234900	82846.036904	59.684506
2300.260563	82692.750133	59.689511
2300.015672	82524.777438	59.694516
2299.499808	82369.284371	59.699521
2298.559821	82214.594930	59.704525
2298.071945	82046.702627	59.709530
2297.238262	81881.572808	59.714535
2296.759337	81718.251371	59.719540
2295.868942	81557.823139	59.724545
2295.458544	81398.169280	59.729549
2294.730496	81234.244683	59.734554
2293.711909	81079.347956	59.739559
2293.478363	80909.212609	59.744564
2292.497135	80757.094580	59.749569
2291.544000	80591.170041	59.754573
2291.013513	80431.650377	59.759578
2290.553955	80270.897564	59.764583
2289.899260	80118.985924	59.769588
2289.122676	79967.417933	59.774593
2288.492023	79799.712150	59.779597
2287.522204	79639.121212	59.784602
2286.799375	79492.364489	59.789607
2286.593608	79328.283400	59.794612
2285.970827	79184.916047	59.799617
2285.251443	79019.207853	59.804621
2284.737350	78862.390944	59.809626
2284.065637	78691.950412	59.814631
2283.638677	78529.970270	59.819636
2282.666265	78375.872249	59.824641
2282.091760	78214.380586	59.829645
2281.768811	78052.907329	59.834650
2280.645877	77898.203094	59.839655
2280.192858	77721.367541	59.844660
2279.499620	77561.091149	59.849665
2279.214375	77401.239222	59.854669
2278.399863	77226.024078	59.859674
2277.785120	77069.300212	59.864679
2276.963160	76901.635757	59.869684
2276.133084	76735.032141	59.874689
2275.622585	76565.965073	59.879693
2275.036769	76406.675516	59.884698
2274.057338	76255.826096	59.889703
2273.425594	76078.038355	59.894708
2272.870073	75924.722763	59.899713
2272.003982	75754.001768	59.904718
2271.350462	75602.978794	59.909722
2270.224322	75440.791928	59.914727
2270.041522	75275.713303	59.919732
2269.182081	75124.314731	59.924737
2268.598159	74960.335046	59.929742
2268.350873	74799.876663	59.934746
2267.306650	74639.197491	59.939751
2266.954617	74472.511330	59.944756
2266.119170	74322.280736	59.949761
2265.534059	74150.755797	59.954766
2264.890260	73988.187345	59.959770
2264.267518	73826.833275	59.964775
2263.710666	73666.236634	59.969780
2263.011466	73518.277525	59.974785
2262.290562	73351.355078	59.979790
2261.763684	73185.968054	59.984794
2260.958487	73022.451075	59.989799
2260.730851	72849.746576	59.994804
2259.873006	72684.169129	59.999809
2259.130143	72523.687189	60.004814
2258.477501	72361.456448	60.009818
2257.697438	72193.628159	60.014823
2257.521888	72018.236593	60.019828
2256.410200	71869.968707	60.024833
2255.602303	71694.984361	60.029838
2255.241776	71526.239975	60.034842
2254.501167	71364.265712	60.039847
2253.710242	71200.444715	60.044852
2252.776711	71038.427702	60.049857
2252.441928	70874.423034	60.054862
2251.766758	70711.404879	60.059866
2250.989299	70557.196442	60.064871
2250.627412	70390.539641	60.069876
2249.722755	70227.916604	60.074881
2249.051825	70050.378704	60.079886
2248.543705	69890.406614	60.084890
2247.796276	69721.967039	60.089895
2247.004435	69563.980853	60.094900
2246.492345	69400.668984	60.099905
2246.161805	69232.769215	60.104910
2244.916041	69068.556712	60.109914
2244.440735	68905.122792	60.114919
2244.090626	68733.151397	60.119924
2243.316035	68579.053046	60.124929
2242.359990	68409.429095	60.129934
2241.786737	68245.750208	60.134938
2240.894556	68083.073322	60.139943
2240.567638	67919.085760	60.144948
2239.476198	67767.248157	60.149953
2238.976065	67595.247252	60.154958
2238.508363	67436.574513	60.159962
2237.658228	67270.819721	60.164967
2237.369351	67107.301636	60.169972
2236.859518	66936.270764	60.174977
2235.779040	66776.623968	60.179982
2235.544612	66618.063419	60.184986
2234.451652	66445.492262	60.189991
2233.978751	66278.489177	60.194996
2233.479356	66114.778543	60.200001
2232.818704	65944.936125	60.205006
2231.893283	65793.382148	60.210010
2231.073835	65622.434178	60.215015
2230.785828	65448.259223	60.220020
2229.888695	65286.350721	60.225025
2229.249805	65114.796014	60.230030
2228.823933	64960.269019	60.235034
2228.169536	64792.857991	60.240039
2227.480626	64622.784763	60.245044
2226.807315	64464.682003	60.250049
2226.119428	64284.327773	60.255054
2225.561001	64110.812590	60.260058
2224.699909	63947.446922	60.265063
2224.082469	63774.045473	60.270068
2223.392233	63609.142206	60.275073
2223.137020	63445.276309	60.280078
2222.132632	63278.589430	60.285082
2221.298067	63110.047135	60.290087
2220.594740	62941.897091	60.295092
2219.804026	62781.252985	60.300097
2219.587638	62617.283584	60.305102
2218.462759	62448.343653	60.310106
2217.802605	62287.879299	60.315111
2217.188068	62119.507181	60.320116
2216.473127	61962.751950	60.325121
2215.876656	61800.119392	60.330126
2215.265062	61634.799754	60.335130
2214.352095	61478.960023	60.340135
2214.055137	61311.560920	60.345140
2213.265872	61154.412649	60.350145
2212.638743	60992.045170	60.355150
2212.258856	60831.650031	60.360154
2211.298300	60669.265418	60.365159
2210.839558	60505.954241	60.370164
2209.926690	60334.407029	60.375169
2209.532686	60175.434716	60.380174
2208.612348	60012.099761	60.385178
2208.120060	59848.426103	60.390183
2207.370018	59683.120260	60.395188
2206.651500	59518.143242	60.400193
2205.911171	59350.626196	60.405198
2205.375764	59190.481842	60.410202
2204.777764	59035.258172	60.415207
2204.472075	58863.026728	60.420212
2203.527818	58696.655748	60.425217
2202.981136	58525.513348	60.430222
2202.267226	58363.590747	60.435226
2201.802087	58189.428412	60.440231
2200.895085	58025.342771	60.445236
2200.038628	57865.238590	60.450241
2199.636478	57693.064932	60.455246
2198.986159	57527.866850	60.460250
2198.356060	57367.006271	60.465255
2197.492191	57202.550767	60.470260
2196.864692	57039.638545	60.475265
2196.422491	56875.717236	60.480270
2195.498159	56709.857821	60.485274
2194.837904	56539.770876	60.490279
2194.345318	56366.035154	60.495284
2193.744639	56209.344930	60.500289
2192.925809	56046.012939	60.505294
2192.563930	55870.938273	60.510298
2191.502418	55710.046654	60.515303
2191.153597	55530.805206	60.520308
2190.395986	55365.282749	60.525313
2189.444116	55205.634537	60.530318
2189.123167	55042.241990	60.535322
2188.203444	54883.227578	60.540327
2188.011597	54707.175013	60.545332
2187.177628	54547.491689	60.550337
2186.315131	54368.602597	60.555342
2185.997310	54203.609483	60.560346
2185.093527	54039.213963	60.565351
2184.514772	53869.990101	60.570356
2183.557225	53703.410040	60.575361
2183.379414	53539.824699	60.580366
2182.836009	53366.378661	60.585370
2181.871217	53200.807448	60.590375
2181.253018	53023.319924	60.595380
2180.491629	52866.750311	60.600385
2180.112448	52691.117172	60.605390
2179.783472	52516.835204	60.610394
2178.582894	52340.826338	60.615399
2178.053703	52168.357740	60.620404
2177.232898	51999.455516	60.625409
2176.782140	51826.781564	60.630414
2175.875068	51656.871078	60.635418
2175.194121	51488.356450	60.640423
2174.465460	51312.852271	60.645428
2173.962269	51163.454495	60.650433
2173.230010	50979.680435	60.655438
2172.960298	50811.787145	60.660442
2172.116853	50639.164738	60.665447
2171.792911	50462.918101	60.670452
2170.863159	50303.711388	60.675457
2170.373544	50116.914729	60.680462
2169.921289	49942.186864	60.685466
2168.693828	49765.242555	60.690471
2168.409008	49590.918659	60.695476
2167.548189	49424.698164	60.700481
2166.584126	49253.231360	60.705486
2166.103892	49072.853593	60.710490
2165.325214	48910.177557	60.715495
2164.624133	48732.318493	60.720500
2164.059018	48569.444026	60.725505
2163.569117	48391.871214	60.730510
2162.861605	48221.901600	60.735514
2161.845907	48051.324523	60.740519
2161.791161	47879.888041	60.745524
2160.813105	47699.736056	60.750529
2159.813801	47531.815415	60.755534
2159.349515	47359.784650	60.760538
2158.519090	47192.564827	60.765543
2158.083401	47025.903952	60.770548
2157.000490	46862.972334	60.775553
2156.401932	46699.022761	60.780558
2156.242437	46525.259492	60.785562
2155.276438	46368.111897	60.790567
2155.049611	46202.115230	60.795572
2154.112241	46027.822367	60.800577
2153.326997	45850.258703	60.805582
2152.747979	45678.582022	60.810586
2151.945473	45522.194149	60.815591
2151.528783	45353.006274	60.820596
2150.774573	45182.753924	60.825601
2150.111903	45004.268477	60.830606
2149.219952	44834.876358	60.835610
2148.364904	44667.630717	60.840615
2148.250055	44501.774713	60.845620
2147.482491	44333.689753	60.850625
2146.639834	44169.536901	60.855630
2146.075115	44007.460484	60.860634
2145.412415	43840.299796	60.865639
2144.428346	43659.491319	60.870644
2143.452881	43500.612604	60.875649
2143.029577	43348.991160	60.880654
2142.483622	43182.855590	60.885658
2141.915800	43031.756361	60.890663
2141.253415	42851.673748	60.895668
2140.992230	42683.492788	60.900673
2140.213951	42517.365672	60.905678
2139.644255	42350.400657	60.910682
2138.985491	42177.338604	60.915687
2138.281572	42005.917196	60.920692
2137.265344	41847.717883	60.925697
2136.584770	41675.268321	60.930702
2136.118921	41502.650443	60.935706
2135.413411	41357.384028	60.940711
2134.857116	41186.380571	60.945716
2134.240701	41006.616649	60.950721
2133.466642	40845.403097	60.955726
2132.742168	40681.463826	60.960730
2132.153767	40515.442893	60.965735
2131.595671	40335.961326	60.970740
2130.966687	40179.638425	60.975745
2130.502263	40009.269261	60.980750
2129.888808	39836.293159	60.985754
2129.173220	39667.666769	60.990759
2128.450377	39494.436402	60.995764
2127.747187	39326.385290	61.000769
2127.166701	39154.030584	61.005774
2126.527762	38981.003960	61.010778
2125.751969	38807.524971	61.015783
2124.990397	38629.355152	61.020788
2124.320307	38472.969051	61.025793
2123.879890	38287.491144	61.030798
2123.067171	38126.306249	61.035802
2122.126739	37952.074888	61.040807
2121.621120	37780.533170	61.045812
2120.802018	37617.811306	61.050817
2120.341752	37456.815551	61.055822
2119.367490	37286.450225	61.060826
2119.287798	37120.449661	61.065831
2118.617792	36937.781280	61.070836
2118.065900	36779.590092	61.075841
2117.041345	36599.967501	61.080846
2116.350992	36421.940815	61.085850
2115.905384	36269.344053	61.090855
2115.297273	36089.649766	61.095860
2114.409873	35921.280756	61.100865
2113.591468	35746.354196	61.105870
2112.939911	35580.091275	61.110874
2112.100584	35418.160435	61.115879
2111.796461	35246.531931	61.120884
2110.839067	35087.539081	61.125889
2109.925885	34913.984417	61.130894
2109.940715	34747.059793	61.135898
2109.050274	34592.100720	61.140903
2108.394596	34415.901034	61.145908
2107.798748	34248.267522	61.150913
2107.010332	34081.015521	61.155918
2106.811092	33910.860192	61.160922
2105.856380	33740.380806	61.165927
2105.209981	33568.248599	61.170932
2104.452277	33411.896624	61.175937
2103.683107	33235.487221	61.180942
2103.024557	33069.929955	61.185946
2102.429783	32894.477879	61.190951
2101.657217	32735.090985	61.195956
2101.075761	32570.669016	61.200961
2100.302716	32400.166670	61.205966
2099.720735	32229.687911	61.210970
2099.080873	32070.793613	61.215975
2098.532674	31894.063191	61.220980
2097.803460	31737.041439	61.225985
2097.066905	31559.330008	61.230990
2096.717396	31393.530320	61.235994
2095.777227	31232.345220	61.240999
2095.289306	31061.640803	61.246004
2094.678318	30887.739010	61.251009
2093.759702	30717.008545	61.256014
2093.413821	30553.215559	61.261018
2092.266445	30384.717991	61.266023
2092.121814	30212.983541	61.271028
2091.364607	30047.282662	61.276033
2090.406661	29880.035305	61.281038
2090.066574	29720.585259	61.286042
2089.405992	29555.739860	61.291047
2088.719887	29374.048315	61.296052
2087.919021	29215.889716	61.301057
2087.182205	29025.575701	61.306062
2086.987721	28865.134502	61.311066
2085.890284	28698.430111	61.316071
2085.241198	28524.940222	61.321076
2084.484701	28363.228132	61.326081
2083.614127	28199.064874	61.331086
2083.352225	28029.740174	61.336090
2082.583503	27857.873593	61.341095
2082.232482	27698.813152	61.346100
2081.420104	27523.857475	61.351105
2080.591126	27349.110109	61.356110
2080.027035	27184.758402	61.361114
2079.234888	27026.586548	61.366119
2078.616229	26850.102717	61.371124
2078.195418	26683.269803	61.376129
2077.325980	26513.095320	61.381134
2076.581659	26344.248653	61.386138
2075.770464	26176.922140	61.391143
2075.467704	26004.038518	61.396148
2074.203223	25844.199815	61.401153
2073.896755	25681.932893	61.406158
2073.424112	25519.433345	61.411162
2072.437128	25361.487237	61.416167
2071.969151	25181.947615	61.421172
2071.195276	25022.378049	61.426177
2070.357451	24854.916305	61.431182
2070.096902	24680.482813	61.436186
2069.355728	24535.637024	61.441191
2068.782501	24367.753779	61.446196
2067.599594	24208.560488	61.451201
2067.103709	24031.420004	61.456206
2066.560432	23864.334907	61.461210
2065.782532	23708.428336	61.466215
2065.412752	23551.686992	61.471220
2064.409115	23386.644714	61.476225
2063.655960	23219.467012	61.481230
2063.138375	23054.026492	61.486234
2061.918430	22895.526572	61.491239
2061.954005	22730.285914	61.496244
2060.960533	22582.322705	61.501249
2060.089852	22421.099929	61.506254
2059.733559	22253.935731	61.511258
2058.812465	22101.749683	61.516263
2058.434044	21940.052549	61.521268
2057.470998	21790.320799	61.526273
2056.797429	21631.739699	61.531278
2056.466817	21473.709801	61.536282
2055.550741	21322.069746	61.541287
2055.147923	21166.171256	61.546292
2054.024680	21012.843403	61.551297
2053.426509	20851.696018	61.556302
2052.962791	20697.648339	61.561306
2052.055079	20545.228820	61.566311
2051.566966	20392.601282	61.571316
2051.059315	20244.010850	61.576321
2049.843860	20078.279136	61.581326
2049.008432	19940.487013	61.586330
2047.858031	19800.332166	61.591335
2047.092987	19661.319036	61.596340
2046.424005	19531.434236	61.601345
2045.627741	19397.953279	61.606350
2044.823370	19269.903218	61.611354
2043.982501	19140.408942	61.616359
2043.366428	19015.826082	61.621364
2042.599997	18890.185328	61.626369
2041.787678	18764.855229	61.631374
2040.999034	18656.048722	61.636378
2040.526274	18531.375139	61.641383
2039.861944	18409.466776	61.646388
2038.502515	18306.144367	61.651393
2038.007037	18190.340077	61.656398
2037.379901	18081.321301	61.661402
2036.532751	17967.661312	61.666407
2035.478801	17862.396798	61.671412
2034.915717	17759.244115	61.676417
2034.116315	17661.818035	61.681422
2033.207051	17569.965766	61.686426
2032.475119	17481.952727	61.691431
2031.886556	17375.646701	61.696436
2031.163015	17291.767815	61.701441
2030.380091	17200.589573	61.706446
2029.778715	17106.231092	61.711450
2029.038093	17018.942558	61.716455
2028.551864	16929.095481	61.721460
2027.835334	16840.237047	61.726465
2027.127137	16743.747908	61.731470
2026.236571	16661.681300	61.736474
2025.432545	16576.335479	61.741479
2025.354797	16486.175130	61.746484
2024.686012	16411.055185	61.751489
2023.671328	16325.641962	61.756494
2023.221934	16235.512850	61.761498
2022.199671	16151.001629	61.766503
2021.742495	16065.813932	61.771508
2021.303705	15982.701855	61.776513
2020.900941	15894.268305	61.781518
2019.920924	15818.105670	61.786522
2019.303880	15731.977104	61.791527
2018.583449	15632.899447	61.796532
2018.275733	15558.843593	61.801537
2017.301099	15470.192057	61.806542
2016.931735	15373.573640	61.811546
2015.806874	15284.969114	61.816551
2015.280566	15206.050003	61.821556
2014.394801	15122.450552	61.826561
2013.805527	15046.664410	61.831566
2013.108897	14961.453928	61.836570
2012.459281	14892.930852	61.841575
2012.067357	14801.836721	61.846580
2011.249707	14723.555701	61.851585
2010.444515	14641.994576	61.856590
2010.051672	14562.902792	61.861594
2009.447612	14482.740993	61.866599
2009.005313	14382.569764	61.871604
2008.182533	14315.833579	61.876609
2007.462799	14232.011471	61.881614
2007.129158	14148.650118	61.886618
2006.230053	14069.764272	61.891623
2005.839836	13979.233713	61.896628
2005.133188	13886.826666	61.901633
2004.373381	13803.895298	61.906638
2003.863049	13712.069286	61.911642
2002.786479	13630.900411	61.916647
2002.284457	13550.184724	61.921652
2001.415696	13468.394006	61.926657
2000.790314	13375.715041	61.931662
2000.339166	13293.990743	61.936666
1999.229395	13221.400859	61.941671
1998.717521	13145.659775	61.946676
1998.293202	13058.209354	61.951681
1997.546525	12981.009507	61.956686
1997.646208	12903.227081	61.961690
1996.716688	12809.431776	61.966695
1995.880701	12719.812375	61.971700
1995.171204	12644.279351	61.976705
1994.576165	12553.055845	61.981710
1994.158271	12461.504502	61.986714
1992.954305	12392.073487	61.991719
1992.653809	12294.717035	61.996724
1991.717958	12211.817332	62.001729
1991.057549	12149.845541	62.006734
1990.651852	12056.663986	62.011738
1989.787540	11975.113072	62.016743
1989.297387	11885.848506	62.021748
1988.554302	11812.015207	62.026753
1987.728117	11715.731881	62.031758
1987.544307	11636.096043	62.036762
1986.968564	11554.967148	62.041767
1986.380931	11463.805421	62.046772
1985.588346	11377.103891	62.051777
1984.782090	11294.914973	62.056782
1984.230025	11202.240860	62.061786
1983.583688	11119.631793	62.066791
1982.912956	11030.976146	62.071796
1981.957762	10951.316025	62.076801
1981.415598	10861.114539	62.081806
1981.082871	10767.135140	62.086810
1979.939780	10700.408252	62.091815
1979.401625	10611.004159	62.096820
1979.017811	10520.260778	62.101825
1978.101478	10429.138518	62.106830
1977.534916	10351.621065	62.111834
1976.679072	10260.496140	62.116839
1976.281192	10176.741849	62.121844
1975.479906	10103.322213	62.126849
1974.803646	10020.616992	62.131854
1974.431457	9927.244781	62.136858
1973.483822	9844.955613	62.141863
1972.771690	9753.664976	62.146868
1972.211594	9664.516926	62.151873
1971.358853	9578.719724	62.156878
1970.396856	9506.383380	62.161882
1969.693899	9422.410296	62.166887
1969.420956	9348.851698	62.171892
1968.790953	9280.256331	62.176897
1967.783005	9189.688272	62.181902
1967.698500	9111.727699	62.186906
1966.640624	9031.376866	62.191911
1966.165752	8945.906728	62.196916
1965.701472	8869.320902	62.201921
1964.680530	8785.391203	62.206926
1964.142561	8700.172319	62.211930
1963.438355	8622.509490	62.216935
1962.771630	8527.951724	62.221940
1962.362139	8456.254612	62.226945
1961.512807	8382.222241	62.231950
1960.986400	8292.595348	62.236954
1959.992434	8210.855407	62.241959
1959.279766	8132.338522	62.246964
1958.572190	8057.330284	62.251969
1957.754195	7983.846749	62.256974
1957.505682	7900.114962	62.261978
1956.930667	7835.551101	62.266983
1956.397704	7734.699111	62.271988
1955.473972	7657.535270	62.276993
1954.499097	7576.226501	62.281998
1954.306528	7491.879104	62.287002
1953.609569	7424.509843	62.292007
1952.958614	7342.911110	62.297012
1952.083910	7255.068215	62.302017
1951.340397	7184.716854	62.307022
1950.898325	7108.223684	62.312026
1949.687491	7031.748417	62.317031
1949.505558	6952.488094	62.322036
1948.942028	6881.797211	62.327041
1947.940784	6812.474573	62.332046
1947.595143	6726.373816	62.337050
1946.460777	6656.230565	62.342055
1946.207795	6568.715839	62.347060
1945.498118	6505.105987	62.352065
1944.408180	6438.718602	62.357070
1943.788661	6344.462190	62.362074
1943.164340	6287.398705	62.367079
1942.723454	6200.429489	62.372084
1941.976432	6135.478291	62.377089
1940.977393	6064.768926	62.382094
1940.541986	5983.220735	62.387098
1939.519148	5924.283842	62.392103
1939.148182	5857.898512	62.397108
1938.151645	5793.400959	62.402113
1937.611270	5717.617184	62.407118
1937.006278	5648.138488	62.412122
1935.851191	5585.851918	62.417127
1934.981872	5528.666971	62.422132
1934.621295	5475.848552	62.427137
1933.864126	5415.126762	62.432142
1933.318884	5359.209049	62.437146
1932.491267	5298.684279	62.442151
1931.827351	5234.399019	62.447156
1931.217784	5165.663166	62.452161
1930.553945	5116.850544	62.457166
1930.090630	5061.445469	62.462170
1929.470083	5005.619922	62.467175
1928.818292	4941.058742	62.472180
1927.964013	4878.603574	62.477185
1927.232432	4830.890319	62.482190
1926.677115	4767.847878	62.487194
1925.916681	4708.407254	62.492199
1925.241582	4649.280643	62.497204
1924.561287	4594.293508	62.502209
1923.837113	4539.125041	62.507214
1923.366358	4484.437102	62.512218
1922.807186	4437.231711	62.517223
1922.332906	4377.921299	62.522228
1921.560688	4318.305083	62.527233
1920.713900	4257.034419	62.532238
1920.092720	4194.761250	62.537242
1919.349235	4141.475231	62.542247
1918.727926	4080.652977	62.547252
1917.791345	4030.225479	62.552257
1917.078249	3975.775073	62.557262
1916.560974	3909.368093	62.562266
1915.734798	3868.630744	62.567271
1915.235311	3811.417410	62.572276
1914.494098	3767.191149	62.577281
1914.101687	3717.217004	62.582286
1913.825115	3654.342499	62.587290
1912.849387	3600.356328	62.592295
1912.319924	3539.982312	62.597300
1911.599395	3491.856811	62.602305
1910.752375	3430.413760	62.607310
1910.241130	3367.371109	62.612314
1909.545764	3316.648304	62.617319
1909.048282	3260.796432	62.622324
1908.542508	3199.442131	62.627329
1907.477209	3139.806249	62.632334
1906.835068	3084.470916	62.637338
1906.085912	3027.431977	62.642343
1905.635929	2969.408867	62.647348
1905.008351	2919.432975	62.652353
1904.346048	2856.038749	62.657358
1903.672071	2804.107724	62.662362
1902.563951	2756.457834	62.667367
1902.088725	2698.698473	62.672372
1901.817123	2638.928376	62.677377
1901.020726	2586.854313	62.682382
1900.316569	2533.953525	62.687386
1899.930184	2481.768216	62.692391
1899.265271	2422.369001	62.697396
1898.384180	2359.719827	62.702401
1897.734593	2315.111977	62.707406
1896.915602	2251.833570	62.712410
1895.979509	2200.281456	62.717415
1895.658221	2142.928844	62.722420
1895.228710	2084.469903	62.727425
1894.051017	2036.439909	62.732430
1893.487219	1981.487449	62.737434
1892.689951	1930.810864	62.742439
1892.017382	1878.084079	62.747444
1891.555781	1830.888153	62.752449
1890.924566	1782.791950	62.757454
1890.276704	1730.643740	62.762458
1889.165827	1680.490956	62.767463
1888.624125	1630.091058	62.772468
1888.347688	1575.201750	62.777473
1887.466263	1532.482272	62.782478
1887.034725	1480.250935	62.787482
1886.252228	1441.513982	62.792487
1885.372707	1380.358342	62.797492
1884.878609	1329.490626	62.802497
1884.213324	1291.328450	62.807502
1883.724506	1226.238106	62.812506
1882.746177	1193.352327	62.817511
1882.011919	1135.133249	62.822516
1881.731663	1094.775109	62.827521
1881.039035	1051.350511	62.832526
1880.434408	997.304806	62.837530
1879.576400	941.608934	62.842535
1878.960660	893.200172	62.847540
1878.209825	847.673766	62.852545
1877.495300	795.721640	62.857550
1877.026071	744.591811	62.862554
1876.300957	701.219153	62.867559
1875.540292	650.676844	62.872564
1874.876191	610.171249	62.877569
1874.095789	559.026821	62.882574
1873.506935	509.161072	62.887578
1872.746388	467.184867	62.892583
1872.084484	419.012104	62.897588
1871.251965	383.327937	62.902593
1870.492162	338.998333	62.907598
1870.357698	300.136310	62.912602
1869.124231	259.096037	62.917607
1868.396809	214.927254	62.922612
1867.441240	178.868887	62.927617
1867.016448	138.320310	62.932622
1866.203642	97.104898	62.937626
1865.451074	79.849723	62.942631
1864.802565	46.314948	62.947636
1864.288845	9.727958	62.952641
1863.230513	-20.057846	62.957646
1862.540399	-55.933846	62.962650
1858.374826	14.813433	62.967655
1856.658694	35.756778	62.972660
1857.385730	29.972439	62.977665
1857.535304	38.447097	62.982670
1857.838161	17.080475	62.987674
1857.847988	29.906037	62.992679
1856.462264	29.780934	62.997684
1855.488848	32.099292	63.002689
1854.445336	43.482047	63.007694
1853.991271	38.008239	63.012698
1853.500961	52.576913	63.017703
1853.144749	47.685229	63.022708
1852.830693	50.540718	63.027713
1851.569231	54.645769	63.032718
1851.130058	58.382141	63.037722
1850.252026	55.730578	63.042727
1850.308875	57.093728	63.047732
1849.912698	48.623980	63.052737
1848.368087	52.089594	63.057742
1848.044199	46.815887	63.062746
1847.282851	53.598042	63.067751
1846.442308	55.210912	63.072756
1845.665991	53.549296	63.077761
1844.852430	51.658628	63.082766
1845.158433	52.263127	63.087770
1843.975960	52.616690	63.092775
1844.089053	46.598665	63.097780
1842.856569	45.523567	63.102785
1841.757706	58.089954	63.107790
1841.593662	53.509955	63.112794
1841.153212	59.228759	63.117799
1840.375245	58.243918	63.122804
1839.558317	59.630691	63.127809
1838.775718	68.169799	63.132814
1838.392146	56.840609	63.137818
1837.786854	64.501585	63.142823
1836.969310	64.976979	63.147828
1836.297916	61.338553	63.152833
1835.457544	63.411870	63.157838
1834.996874	53.094714	63.162842
1834.365206	57.774708	63.167847
1833.334900	60.590966	63.172852
1832.993814	59.010055	63.177857
1831.914710	63.548209	63.182862
1831.752031	60.653754	63.187866
1831.008912	65.477603	63.192871
1830.307999	63.644746	63.197876
1829.585190	58.256186	63.202881
1828.730993	62.034808	63.207886
1828.293870	57.789907	63.212890
1827.457993	65.578962	63.217895
1826.923238	61.699646	63.222900
1826.300918	64.101041	63.227905
1825.965770	65.381356	63.232910
1825.149576	66.405318	63.237914
1824.369438	60.127000	63.242919
1823.863834	60.663252	63.247924
1823.401023	59.249905	63.252929
1822.298524	61.987744	63.257934
1822.267886	57.042788	63.262938
1821.091236	69.410230	63.267943
1820.762745	64.358026	63.272948
1820.060146	64.534476	63.277953
1819.405294	61.481632	63.282958
1819.090239	56.001521	63.287962
1818.368351	65.492931	63.292967
1817.375081	67.781344	63.297972
1816.086539	64.829125	63.302977
1815.971048	55.217252	63.307982
1815.809573	56.129368	63.312986
1814.280867	54.735468	63.317991
1813.475606	64.822012	63.322996
1813.552667	53.594729	63.328001
1812.741135	61.360996	63.333006
1812.108701	54.899958	63.338010
1810.957998	62.944011	63.343015
1810.625752	57.392514	63.348020
1810.118653	59.023410	63.353025
1809.077977	64.121595	63.358030
1808.634983	59.525970	63.363034
1808.136236	60.964729	63.368039
1807.855434	57.787837	63.373044
1807.159911	55.433737	63.378049
1806.357203	62.336013	63.383054
1805.980428	58.277076	63.388058
1804.886322	60.953665	63.393063
1803.769743	57.849568	63.398068
1803.123577	56.692422	63.403073
1802.925068	63.312674	63.408078
1802.534049	54.703343	63.413082
1801.687559	67.595525	63.418087
1800.499568	60.673930	63.423092
1799.657111	68.096608	63.428097
1799.052669	61.643742	63.433102
1798.421407	54.745708	63.438106
1797.860653	54.943793	63.443111
1798.237820	55.267327	63.448116
1797.618703	58.609657	63.453121
1796.711422	65.918050	63.458126
1795.999632	60.280170	63.463130
1794.844025	61.635583	63.468135
1793.540852	53.150605	63.473140
1793.729104	59.565935	63.478145
1792.942034	64.054574	63.483150
1792.262496	50.041123	63.488154
1791.550609	60.768852	63.493159
1790.922283	67.525170	63.498164
1790.444653	58.227850	63.503169
1789.670788	63.278941	63.508174
1789.323406	56.458830	63.513178
1788.899595	65.844562	63.518183
1788.001985	56.718017	63.523188
1786.692599	55.253036	63.528193
1785.789823	58.331333	63.533198
1785.361270	56.866821	63.538202
1785.045420	56.442546	63.543207
1784.896404	60.940247	63.548212
1783.936949	57.789130	63.553217
1782.941260	69.711532	63.558222
1782.949281	51.025200	63.563226
1782.397618	62.438691	63.568231
1780.941285	55.261680	63.573236
1780.289875	59.096420	63.578241
1779.275639	68.657919	63.583246
1778.987220	60.926428	63.588250
1778.255797	64.009056	63.593255
1778.018162	57.139979	63.598260
1777.404454	57.398517	63.603265
1776.771980	63.688718	63.608270
1776.366573	57.071789	63.613274
1775.196033	60.134265	63.618279
1774.243133	61.466957	63.623284
1773.660137	57.541701	63.628289
1773.067871	57.085630	63.633294
1772.494211	48.981554	63.638298
1771.761125	63.347522	63.643303
1771.473577	59.299653	63.648308
1771.080464	55.863059	63.653313
1770.250329	63.551866	63.658318
1769.678243	61.171866	63.663322
1768.251431	58.634293	63.668327
1767.606089	58.342771	63.673332
1767.395991	59.568539	63.678337
1766.725283	69.707844	63.683342
1766.123245	65.430798	63.688346
1765.822708	57.430000	63.693351
1764.662196	58.499200	63.698356
1763.852884	58.345683	63.703361
1762.877183	59.488035	63.708366
1762.723471	54.953713	63.713370
1762.154350	54.352044	63.718375
1761.318315	51.143490	63.723380
1761.331112	56.962207	63.728385
1760.154287	53.553885	63.733390
1759.537072	60.489790	63.738394
1758.702862	62.007065	63.743399
1758.151199	57.382979	63.748404
1757.627859	60.257523	63.753409
1757.082199	70.190889	63.758414
1756.301394	66.740173	63.763418
1754.949170	61.547792	63.768423
1754.736625	60.287100	63.773428
1753.938164	58.091289	63.778433
1753.235023	68.305132	63.783438
1753.279018	54.858027	63.788442
1752.439882	66.384988	63.793447
1751.498217	68.351416	63.798452
1750.406301	65.858435	63.803457
1749.751963	69.985385	63.808462
1749.340575	64.460659	63.813466
1748.577137	70.232349	63.818471
1748.404377	69.069417	63.823476
1748.171967	61.828930	63.828481
1747.386687	73.945009	63.833486
1746.687032	52.166710	63.838490
1745.303076	55.365593	63.843495
1744.648662	63.378158	63.848500
1744.323422	57.406093	63.853505
1743.335292	68.251824	63.858510
1743.203811	56.825853	63.863514
1742.250691	59.440652	63.868519
1741.377363	53.800063	63.873524
1740.849916	57.391196	63.878529
1740.059344	67.629965	63.883534
1739.836086	62.100594	63.888538
1739.312012	62.455292	63.893543
1738.907551	60.171679	63.898548
1737.689836	59.264596	63.903553
1736.710754	64.559604	63.908558
1736.195374	58.605123	63.913562
1735.674888	67.233508	63.918567
1735.021620	59.265083	63.923572
1734.661878	62.045839	63.928577
1733.818558	64.523354	63.933582
1732.952946	53.493106	63.938586
1732.045097	69.755527	63.943591
1731.660806	62.454009	63.948596
1731.504787	64.579514	63.953601
1730.759089	61.662549	63.958606
1729.793710	48.134494	63.963610
1728.968737	56.456421	63.968615
1728.152657	66.245081	63.973620
1727.769070	59.137419	63.978625
1727.239660	64.534475	63.983630
1727.005109	56.236201	63.988634
1725.817429	61.621112	63.993639
1724.787929	57.568090	63.998644
1723.983743	58.703716	64.003649
1723.587345	62.936358	64.008654
1723.371485	56.193142	64.013658
1722.578218	64.440653	64.018663
1722.260249	61.840531	64.023668
1721.709620	60.843274	64.028673
1720.411611	67.338539	64.033678
1720.053638	61.895223	64.038682
1719.342603	63.790337	64.043687
1718.332866	59.729447	64.048692
1717.483823	56.092466	64.053697
1716.644523	68.810059	64.058702
1716.315651	51.642235	64.063706
1715.642039	60.324902	64.068711
1715.470670	62.093301	64.073716
1714.776244	48.813953	64.078721
1714.556293	68.198283	64.083726
1713.789190	55.543906	64.088730
1712.764970	62.910317	64.093735
1711.981930	61.973630	64.098740
1711.838938	55.594157	64.103745
1710.583874	62.481571	64.108750
1709.866108	60.339189	64.113754
1709.106514	66.208047	64.118759
1708.899815	58.061470	64.123764
1708.404281	51.432066	64.128769
1707.075102	66.767931	64.133774
1706.237023	50.977244	64.138778
1705.355165	51.134888	64.143783
1704.821523	59.338008	64.148788
1704.510430	57.578889	64.153793
1703.637161	65.891151	64.158798
1703.653967	54.429021	64.163802
1702.871414	63.406538	64.168807
1702.589134	63.412179	64.173812
1701.698840	64.566220	64.178817
1700.718870	62.875495	64.183822
1700.316750	54.102373	64.188826
1699.547204	55.842782	64.193831
1698.508221	54.629787	64.198836
1697.808477	59.487776	64.203841
1697.044612	62.594499	64.208846
1696.736035	53.317667	64.213850
1696.064251	56.261530	64.218855
1695.667419	54.426145	64.223860
1695.361057	58.594025	64.228865
1694.331988	59.823726	64.233870
1693.942500	59.310234	64.238874
1693.232913	50.502376	64.243879
1691.720227	58.570850	64.248884
1691.412289	59.540929	64.253889
1690.765015	58.354026	64.258894
1690.339873	59.624996	64.263898
1689.430034	58.785728	64.268903
1688.890814	63.091522	64.273908
1688.307302	56.753639	64.278913
1687.115300	57.982415	64.283918
1686.955292	56.896311	64.288922
1686.507737	63.530891	64.293927
1685.651422	58.141509	64.298932
1685.259314	51.681763	64.303937
1683.854090	56.295424	64.308942
1683.410813	50.241197	64.313946
1682.825650	58.258539	64.318951
1682.234580	55.324914	64.323956
1682.537747	52.853218	64.328961
1680.848035	63.097622	64.333966
1680.203788	53.667531	64.338970
1679.714833	62.726149	64.343975
1679.131129	54.249957	64.348980
1678.090218	53.698018	64.353985
1677.085299	62.067466	64.358990
1676.875767	57.665021	64.363994
1676.290364	55.512664	64.368999
1675.810917	51.430639	64.374004
1675.593250	53.758325	64.379009
1674.515794	56.993713	64.384014
1673.710266	52.512478	64.389018
1672.961483	51.625555	64.394023
1672.454412	50.851625	64.399028
1672.265186	43.060254	64.404033
1670.956752	57.331541	64.409038
1670.601494	46.101987	64.414042
1669.628787	51.771313	64.419047
1668.806587	54.556149	64.424052
1668.172255	45.736349	64.429057
1667.171083	54.754903	64.434062
1666.627853	51.581872	64.439066
1666.183796	50.525122	64.444071
1665.873942	56.347776	64.449076
1665.618378	53.304091	64.454081
1665.008037	54.178707	64.459086
1664.160295	43.462626	64.464090
1663.315019	42.078527	64.469095
1662.554896	54.102298	64.474100
1661.973331	46.847911	64.479105
1660.255984	55.802038	64.484110
1660.120022	54.399880	64.489114
1659.745071	58.126075	64.494119
1659.388422	53.401652	64.499124
1658.714784	53.825855	64.504129
1658.348973	53.037373	64.509134
1657.308313	48.606111	64.514138
1656.516487	52.743878	64.519143
1655.933886	50.206306	64.524148
1655.601108	47.886092	64.529153
1654.168751	56.123172	64.534158
1653.784493	54.694226	64.539162
1652.999625	53.917120	64.544167
1652.560365	54.364017	64.549172
1652.615164	51.873426	64.554177
1650.870677	56.723922	64.559182
1650.292434	60.056636	64.564186
1649.736407	52.118528	64.569191
1649.185155	58.714389	64.574196
1648.958368	54.401423	64.579201
1648.210046	57.991389	64.584206
1647.433549	61.366636	64.589210
1646.750458	60.653788	64.594215
1646.053738	61.319781	64.599220
1645.662120	50.556475	64.604225
1644.088117	57.158690	64.609230
1643.733011	49.535596	64.614234
1643.393693	57.168537	64.619239
1642.737754	55.766982	64.624244
1642.550061	56.285881	64.629249
1641.531874	60.890119	64.634254
1640.975556	63.396186	64.639258
1640.449537	46.735949	64.644263
1639.491975	68.325323	64.649268
1638.642204	46.616666	64.654273
1637.764621	57.107388	64.659278
1637.592907	55.810259	64.664282
1637.002039	54.724797	64.669287
1635.920358	59.834285	64.674292
1635.179393	46.784715	64.679297
1634.449513	62.337630	64.684302
1634.092465	57.693699	64.689306
1633.639485	55.391005	64.694311
1633.205694	55.726651	64.699316
1632.196584	51.653086	64.704321
1631.291465	59.156717	64.709326
1631.189218	55.836368	64.714330
1630.396449	52.919030	64.719335
1629.435407	63.096589	64.724340
1628.777364	53.167239	64.729345
1627.983332	58.402920	64.734350
1627.423105	51.990395	64.739354
1626.639197	53.089711	64.744359
1625.853962	58.071684	64.749364
1625.609575	46.286789	64.754369
1624.909319	58.064517	64.759374
1624.464816	58.505944	64.764378
1623.629893	57.962303	64.769383
1622.515224	56.009158	64.774388
1622.333150	50.542652	64.779393
1621.698071	63.070118	64.784398
1621.202484	51.396090	64.789402
1620.214849	50.977636	64.794407
1619.500873	54.984773	64.799412
1619.228098	50.168187	64.804417
1618.496856	52.987473	64.809422
1617.692616	62.585038	64.814426
1617.258565	57.794071	64.819431
1616.360504	54.127069	64.824436
1616.091368	56.240586	64.829441
1614.725853	58.310665	64.834446
1614.085943	44.637927	64.839450
1613.450580	52.679020	64.844455
1613.118840	51.426240	64.849460
1612.579586	53.737212	64.854465
1611.168319	63.631490	64.859470
1611.044415	49.629189	64.864474
1610.412620	56.636818	64.869479
1609.826477	65.351340	64.874484
1609.372258	58.827359	64.879489
1607.927556	56.638072	64.884494
1607.769169	63.182565	64.889498
1607.341605	56.069303	64.894503
1606.768113	58.068749	64.899508
1605.632209	53.056555	64.904513
1604.795887	59.776560	64.909518
1604.266302	55.568476	64.914522
1603.889170	59.714490	64.919527
1602.849552	54.940888	64.924532
1602.105705	50.877232	64.929537
1600.969249	67.272186	64.934542
1600.700980	48.847408	64.939546
1600.378186	58.330638	64.944551
1599.921636	52.276963	64.949556
1599.808379	40.185818	64.954561
1598.476792	45.172593	64.959566
1597.968693	48.230820	64.964570
1597.510834	44.793510	64.969575
1596.563793	45.907714	64.974580
1595.618649	48.507101	64.979585
1594.658270	58.038012	64.984590
1594.476613	50.131906	64.989594
1594.071014	50.206037	64.994599
1593.264354	54.978532	64.999604
1592.620834	52.521618	65.004609
1591.402361	50.952409	65.009614
1590.986384	52.467941	65.014618
1590.388176	54.720474	65.019623
1590.048489	53.781195	65.024628
1589.596774	44.804676	65.029633
1588.360288	55.648896	65.034638
1587.936539	52.792791	65.039642
1587.198359	50.208992	65.044647
1586.719841	41.452776	65.049652
1585.777322	41.419826	65.054657
1584.779643	52.246603	65.059662
1584.289540	44.895708	65.064666
1583.756100	55.970427	65.069671
1583.263714	46.489439	65.074676
1583.209646	44.192764	65.079681
1581.938952	56.606752	65.084686
1581.311336	46.290969	65.089690
1580.775119	46.049965	65.094695
1580.081328	52.097625	65.099700
1579.224113	44.087549	65.104705
1578.358425	54.516469	65.109710
1578.285895	44.145610	65.114714
1577.429789	46.902743	65.119719
1576.592005	52.361428	65.124724
1575.769526	52.664222	65.129729
1575.192200	50.102179	65.134734
1575.230944	44.546980	65.139738
1574.218640	50.298320	65.144743
1573.016643	48.247111	65.149748
1572.561282	39.906688	65.154753
1571.640220	48.527763	65.159758
1571.366625	45.718767	65.164762
1570.853206	44.556361	65.169767
1569.847421	48.557834	65.174772
1569.510311	39.438535	65.179777
1568.853927	46.073184	65.184782
1568.188783	47.959466	65.189786
1567.818560	50.484861	65.194791
1566.850556	45.130623	65.199796
1566.096994	51.105782	65.204801
1565.405327	60.259694	65.209806
1564.939753	42.571180	65.214810
1563.999161	52.892155	65.219815
1563.231589	57.122287	65.224820
1563.252266	46.618349	65.229825
1562.535942	58.349753	65.234830
1561.501512	44.938416	65.239834
1560.614499	50.554736	65.244839
1559.716377	51.259060	65.249844
1559.793238	43.876434	65.254849
1558.845132	46.369071	65.259854
1558.064901	43.719425	65.264858
1557.698140	51.605884	65.269863
1556.815276	47.242636	65.274868
1556.462052	50.780884	65.279873
1555.000501	53.197411	65.284878
1554.661491	49.498375	65.289882
1554.099736	55.791567	65.294887
1553.745471	62.159025	65.299892
1553.426543	49.167008	65.304897
1552.187238	58.549863	65.309902
1551.588522	49.394860	65.314906
1551.131211	53.436924	65.319911
1550.272358	58.742848	65.324916
1549.623820	50.516697	65.329921
1548.176649	54.867432	65.334926
1548.149015	44.233979	65.339930
1547.698337	51.293262	65.344935
1546.926504	49.686222	65.349940
1546.688087	43.985831	65.354945
1545.604132	56.699741	65.359950
1544.674207	49.188506	65.364954
1544.519176	47.645885	65.369959
1543.503625	57.409502	65.374964
1543.385577	43.332175	65.379969
1543.099183	51.923375	65.384974
1542.336238	54.908567	65.389978
1540.821200	46.001671	65.394983
1540.235732	52.888409	65.399988
1540.210763	41.327291	65.404993
1538.647561	52.614523	65.409998
1538.244926	50.307004	65.415002
1537.522334	42.523136	65.420007
1537.233836	50.591124	65.425012
1536.807526	51.228370	65.430017
1535.584226	49.631571	65.435022
1534.849264	46.940046	65.440026
1534.428533	42.864495	65.445031
1533.998983	43.454948	65.450036
1533.357086	43.923026	65.455041
1532.039287	56.311400	65.460046
1531.889905	48.717143	65.465050
1531.366071	46.156073	65.470055
1530.269356	59.121174	65.475060
1529.424346	46.130761	65.480065
1528.767202	55.441616	65.485070
1528.250171	50.047271	65.490074
1527.681326	54.815110	65.495079
1527.528480	50.613413	65.500084
1527.015742	40.585327	65.505089
1525.957161	49.256651	65.510094
1525.392455	52.117306	65.515098
1524.420186	53.670782	65.520103
1523.604991	58.313766	65.525108
1523.011264	46.134977	65.530113
1522.313470	51.224503	65.535118
1522.109363	40.822524	65.540122
1521.985461	45.585889	65.545127
1520.553263	57.505171	65.550132
1519.887655	38.697295	65.555137
1519.406205	48.406003	65.560142
1518.608722	43.030998	65.565146
1517.836473	43.540293	65.570151
1516.845552	44.855462	65.575156
1516.725590	34.958932	65.580161
1516.021605	45.746938	65.585166
1514.916436	43.743449	65.590170
1514.299588	46.153500	65.595175
1513.608943	42.338463	65.600180
1513.444833	40.937636	65.605185
1512.976942	48.773936	65.610190
1512.072851	50.909513	65.615194
1511.288740	40.248046	65.620199
1510.783135	55.536671	65.625204
1510.473507	49.108013	65.630209
1509.525862	53.270579	65.635214
1509.004344	49.813441	65.640218
1508.078253	44.939844	65.645223
1507.023852	50.600125	65.650228
1506.798869	45.151493	65.655233
1506.058031	47.865099	65.660238
1505.519048	51.011828	65.665242
1504.400675	52.367756	65.670247
1503.641789	58.219199	65.675252
1503.424067	47.368376	65.680257
1502.911062	54.032294	65.685262
1502.455239	51.712734	65.690266
1501.631245	50.621773	65.695271
1500.369371	48.300995	65.700276
1500.280759	48.698503	65.705281
1499.348507	52.628392	65.710286
1498.587010	48.810426	65.715290
1498.151139	47.962139	65.720295
1497.711174	58.910049	65.725300
1497.529371	38.377393	65.730305
1495.666622	52.019315	65.735310
1495.119443	52.114383	65.740314
1494.516130	45.950019	65.745319
1494.113287	40.425578	65.750324
1493.858593	45.239689	65.755329
1492.266711	55.418181	65.760334
1492.107777	49.318814	65.765338
1491.231401	43.208885	65.770343
1490.807468	51.639018	65.775348
1490.814047	55.033363	65.780353
1489.516604	58.923521	65.785358
1489.208369	59.154082	65.790362
1488.399848	52.129777	65.795367
1487.611803	58.813754	65.800372
1487.254956	51.954212	65.805377
1486.201724	59.806271	65.810382
1485.388823	59.446832	65.815386
1484.622479	56.255685	65.820391
1483.777185	62.131905	65.825396
1483.601942	60.882657	65.830401
1482.972533	57.065780	65.835406
1482.470584	54.545396	65.840410
1481.696461	62.545489	65.845415
1480.681592	64.509450	65.850420
1480.163071	51.085549	65.855425
1479.644626	70.468403	65.860430
1479.210202	55.096221	65.865434
1478.481821	60.275775	65.870439
1477.610628	51.411678	65.875444
1477.322889	49.819189	65.880449
1476.339745	60.903888	65.885454
1475.799025	55.054428	65.890458
1474.986236	58.342448	65.895463
1474.270190	68.466923	65.900468
1473.741155	44.923865	65.905473
1472.807930	62.396716	65.910478
1472.327637	59.415578	65.915482
1471.833056	53.863138	65.920487
1470.893406	56.245653	65.925492
1470.280405	53.120028	65.930497
1469.562621	64.052172	65.935502
1468.995216	55.198144	65.940506
1468.598718	59.426097	65.945511
1467.498934	61.012475	65.950516
1467.062095	54.947814	65.955521
1466.188728	63.149763	65.960526
1465.911695	53.445347	65.965530
1465.281370	62.938034	65.970535
1464.487855	59.473669	65.975540
1463.814287	51.898073	65.980545
1463.305469	64.858074	65.985550
1462.417091	57.956854	65.990554
1461.262862	57.027199	65.995559
1460.643583	65.341732	66.000564
1460.407058	52.655184	66.005569
1459.893962	54.105746	66.010574
1459.538556	66.287588	66.015578
1458.664456	52.073386	66.020583
1457.624337	70.190861	66.025588
1457.783890	49.223906	66.030593
1456.341892	61.457010	66.035598
1455.714027	54.247888	66.040602
1455.023062	55.706219	66.045607
1454.429949	69.129051	66.050612
1454.380637	47.906712	66.055617
1453.245056	66.020432	66.060622
1452.798610	57.812654	66.065626
1452.131510	59.152077	66.070631
1450.878146	57.656289	66.075636
1450.468624	56.855862	66.080641
1449.519516	68.196936	66.085646
1449.515366	57.416252	66.090650
1449.000915	62.222770	66.095655
1448.006982	62.631701	66.100660
1447.127500	59.166814	66.105665
1446.433141	60.244067	66.110670
1445.992348	59.650459	66.115674
1445.024440	59.159551	66.120679
1444.395410	57.518808	66.125684
1443.927312	51.112194	66.130689
1443.668362	51.956243	66.135694
1443.056396	61.105394	66.140698
1442.085471	54.040686	66.145703
1441.305158	61.820999	66.150708
1440.938743	51.634058	66.155713
1439.351046	56.382497	66.160718
1438.724033	55.449482	66.165722
1438.620328	57.041561	66.170727
1437.763022	56.080494	66.175732
1437.625619	60.300387	66.180737
1436.981874	55.545943	66.185742
1436.189343	62.634344	66.190746
1435.546397	52.333661	66.195751
1435.042559	66.595429	66.200756
1434.186353	53.444408	66.205761
1433.083857	65.760761	66.210766
1432.606254	57.671480	66.215770
1431.999815	54.172664	66.220775
1431.460660	58.011712	66.225780
1430.581657	47.149315	66.230785
1429.794871	67.938870	66.235790
1429.652230	57.754208	66.240794
1429.144330	61.438480	66.245799
1427.848135	50.645544	66.250804
1426.941677	59.065647	66.255809
1426.176153	60.709300	66.260814
1426.468633	64.908176	66.265818
1426.083329	61.670678	66.270823
1424.980081	57.216351	66.275828
1424.589921	55.133949	66.280833
1423.316833	57.823366	66.285838
1422.415509	54.163266	66.290842
1421.962230	62.047721	66.295847
1421.285778	62.879284	66.300852
1420.752467	57.306204	66.305857
1420.380209	67.230965	66.310862
1419.643758	61.508822	66.315866
1418.802853	60.087841	66.320871
1417.846199	64.562530	66.325876
1418.133102	54.213405	66.330881
1416.582052	60.946135	66.335886
1415.914698	52.377669	66.340890
1415.496047	46.319595	66.345895
1415.241242	55.862983	66.350900
1414.937086	53.267022	66.355905
1413.668162	52.264157	66.360910
1413.033551	53.705656	66.365914
1412.551992	54.820056	66.370919
1411.138670	63.421655	66.375924
1410.832272	47.474070	66.380929
1410.283984	64.032623	66.385934
1410.140660	48.705664	66.390938
1409.397950	54.412631	66.395943
1408.133248	60.126877	66.400948
1407.795541	51.895523	66.405953
1406.983686	61.197876	66.410958
1406.022442	59.712449	66.415962
1405.371112	53.637742	66.420967
1405.144992	58.236010	66.425972
1404.819437	58.918763	66.430977
1403.488282	53.019923	66.435982
1403.040523	56.980066	66.440986
1402.395448	52.001919	66.445991
1401.657646	59.646173	66.450996
1400.974209	50.727034	66.456001
1400.170428	56.544636	66.461006
1399.857169	51.031203	66.466010
1399.455362	56.149402	66.471015
1398.144219	57.253744	66.476020
1397.576271	45.324792	66.481025
1396.751673	57.262663	66.486030
1396.701043	54.839293	66.491034
1395.911591	54.502964	66.496039
1394.586552	52.502938	66.501044
1394.357111	50.986349	66.506049
1393.677168	54.828858	66.511054
1393.290973	57.424622	66.516058
1392.459141	51.187802	66.521063
1391.696702	60.239453	66.526068
1391.559584	50.438699	66.531073
1391.125604	50.337601	66.536078
1389.450738	50.842178	66.541082
1388.900546	49.926927	66.546087
1388.050717	52.998509	66.551092
1388.017772	51.715612	66.556097
1387.385458	52.958058	66.561102
1386.322379	49.558650	66.566106
1385.957051	50.362844	66.571111
1385.356730	64.594217	66.576116
1384.562182	48.490847	66.581121
1383.364830	55.533220	66.586126
1383.292700	52.796303	66.591130
1382.761006	59.270822	66.596135
1381.738564	56.420039	66.601140
1380.895963	54.813262	66.606145
1380.045629	53.758067	66.611150
1379.860931	52.759489	66.616154
1379.653218	59.321279	66.621159
1378.746451	54.406815	66.626164
1378.179452	45.507026	66.631169
1377.450311	57.600037	66.636174
1376.931251	51.792895	66.641178
1375.909584	55.902616	66.646183
1375.339712	55.717468	66.651188
1374.928662	52.603921	66.656193
1373.751878	46.608023	66.661198
1373.179413	52.226434	66.666202
1372.255806	49.306329	66.671207
1371.754561	55.637237	66.676212
1371.708600	49.876317	66.681217
1370.688806	49.964539	66.686222
1369.880721	56.363147	66.691226
1369.245520	51.555327	66.696231
1368.890597	59.624422	66.701236
1367.830176	47.447337	66.706241
1367.056097	61.304209	66.711246
1366.873066	58.425650	66.716250
1366.304717	55.989964	66.721255
1365.461731	57.590755	66.726260
1364.844898	52.288011	66.731265
1363.980489	60.296172	66.736270
1363.751327	57.812875	66.741274
1362.644063	56.472102	66.746279
1361.837160	66.735616	66.751284
1361.731137	53.309259	66.756289
1360.575242	54.310093	66.761294
1360.191668	43.764787	66.766298
1359.179744	60.603619	66.771303
1358.570383	58.297456	66.776308
1358.369331	53.573586	66.781313
1357.487885	49.601272	66.786318
1356.512649	52.459411	66.791322
1356.135597	40.738249	66.796327
1355.401459	48.787198	66.801332
1355.179973	58.896144	66.806337
1354.124752	52.030957	66.811342
1353.156202	51.000873	66.816346
1352.934223	47.590772	66.821351
1352.444216	47.547473	66.826356
1351.479194	49.877291	66.831361
1350.486763	47.825992	66.836366
1349.971923	51.911921	66.841370
1350.067332	49.775996	66.846375
1348.912405	52.558625	66.851380
1348.235541	45.866684	66.856385
1347.336445	55.703305	66.861390
1347.177258	52.108181	66.866394
1346.382603	43.949487	66.871399
1345.284412	50.168715	66.876404
1344.944296	41.480451	66.881409
1344.242175	52.608811	66.886414
1343.933615	46.373980	66.891418
1342.959564	46.959562	66.896423
1342.107949	53.163248	66.901428
1341.874739	58.729310	66.906433
1340.329601	55.928524	66.911438
1340.034979	52.787014	66.916442
1339.636687	54.701891	66.921447
1338.922819	60.092057	66.926452
1338.493977	56.178681	66.931457
1337.685442	61.058775	66.936462
1337.066009	49.958036	66.941466
1336.721575	56.528946	66.946471
1335.347764	51.103703	66.951476
1334.766574	42.259802	66.956481
1334.259955	47.629632	66.961486
1333.661204	47.406507	66.966490
1333.431682	41.201692	66.971495
1332.274861	55.130450	66.976500
1331.508287	56.671796	66.981505
1330.943805	57.903471	66.986510
1330.565774	48.394916	66.991514
1329.574256	45.186006	66.996519
1328.347186	47.716764	67.001524
1328.339335	43.179805	67.006529
1327.718183	48.397534	67.011534
1327.455876	50.312871	67.016538
1326.957613	49.886116	67.021543
1325.458915	57.629274	67.026548
1325.329009	54.378001	67.031553
1324.302650	58.105290	67.036558
1323.397885	40.160267	67.041562
1323.088211	41.889170	67.046567
1322.106124	56.734740	67.051572
1322.262310	49.341090	67.056577
1321.269231	52.932202	67.061582
1320.246196	52.287682	67.066586
1320.218362	45.148792	67.071591
1319.179686	55.807121	67.076596
1318.505907	47.764836	67.081601
1317.812949	49.553099	67.086606
1317.605838	42.314981	67.091610
1316.640704	47.041779	67.096615
1315.432703	52.493160	67.101620
1315.486186	46.844167	67.106625
1314.737204	54.132247	67.111630
1313.738573	50.087118	67.116634
1313.094149	43.514610	67.121639
1312.367005	55.577351	67.126644
1312.401252	44.951436	67.131649
1311.078043	62.481585	67.136654
1310.695603	55.392762	67.141658
1309.959848	47.021291	67.146663
1309.128646	52.997814	67.151668
1308.388752	50.291375	67.156673
1307.375207	49.060306	67.161678
1307.140180	54.366462	67.166682
1306.678612	51.801851	67.171687
1306.291646	50.969477	67.176692
1305.303513	44.757544	67.181697
1304.189460	51.308890	67.186702
1303.907945	46.416475	67.191706
1303.945850	40.172301	67.196711
1302.652519	54.734624	67.201716
1301.917274	43.794240	67.206721
1300.756025	51.800722	67.211726
1300.888499	46.181749	67.216730
1300.426596	42.917033	67.221735
1299.005890	53.883684	67.226740
1299.326494	47.318597	67.231745
1298.066736	53.259181	67.236750
1296.890413	53.137355	67.241754
1296.400047	49.598046	67.246759
1295.543751	48.436597	67.251764
1295.649650	42.137458	67.256769
1294.932173	50.234233	67.261774
1293.890127	52.018081	67.266778
1293.356824	52.142525	67.271783
1292.672989	49.603795	67.276788
1292.258293	38.122026	67.281793
1291.127284	46.331856	67.286798
1290.137939	48.944682	67.291802
1289.966252	38.958638	67.296807
1289.436867	45.574722	67.301812
1289.249620	41.799565	67.306817
1288.191878	56.885828	67.311822
1287.340026	41.625827	67.316826
1287.173292	43.989590	67.321831
1285.923675	52.718174	67.326836
1285.539349	41.772466	67.331841
1284.473110	48.686796	67.336846
1284.169568	43.116649	67.341850
1283.796617	47.195797	67.346855
1282.354564	54.169883	67.351860
1282.357743	46.571907	67.356865
1281.768592	51.991137	67.361870
1281.040997	51.958820	67.366874
1280.217642	46.928634	67.371879
1279.331929	45.834946	67.376884
1279.249733	41.689854	67.381889
1278.127355	56.209236	67.386894
1277.320813	46.197976	67.391898
1277.172177	52.789795	67.396903
1276.316903	60.184672	67.401908
1275.496851	51.432380	67.406913
1274.648201	50.667112	67.411918
1274.001784	49.253104	67.416922
1273.973385	44.847147	67.421927
1273.325254	48.515891	67.426932
1272.848493	52.397083	67.431937
1272.062239	52.006668	67.436942
1270.744199	51.118917	67.441946
1270.344936	48.605909	67.446951
1269.633726	53.607737	67.451956
1268.963613	50.921754	67.456961
1268.021378	50.612911	67.461966
1267.536995	51.186895	67.466970
1267.231585	47.884687	67.471975
1266.060709	48.589903	67.476980
1265.388581	39.680061	67.481985
1264.509847	54.203282	67.486990
1264.000337	52.557776	67.491994
1263.770511	45.752204	67.496999
1263.164091	51.410725	67.502004
1262.494880	47.404702	67.507009
1261.337340	51.531336	67.512014
1261.058383	41.655392	67.517018
1260.672107	44.933998	67.522023
1259.543382	46.971336	67.527028
1259.062431	45.491600	67.532033
1258.266602	55.385939	67.537038
1257.987222	48.641863	67.542042
1257.233973	40.539700	67.547047
1256.190060	44.962079	67.552052
1256.012072	51.411908	67.557057
1255.256983	44.874362	67.562062
1254.294392	50.745635	67.567066
1253.660721	45.666375	67.572071
1252.842864	53.017459	67.577076
1252.612773	47.881911	67.582081
1251.521857	46.062354	67.587086
1250.879795	45.655325	67.592090
1250.338210	39.976382	67.597095
1249.634560	57.862188	67.602100
1249.557320	44.374514	67.607105
1248.661273	51.796378	67.612110
1247.634643	43.151067	67.617114
1247.384543	50.984300	67.622119
1246.557030	54.419803	67.627124
1245.760577	45.525004	67.632129
1244.918976	59.159242	67.637134
1244.774327	59.141472	67.642138
1244.324421	51.626580	67.647143
1243.171775	52.906068	67.652148
1242.503942	49.442299	67.657153
1241.818495	55.927092	67.662158
1241.031341	52.207908	67.667162
1240.769546	48.635420	67.672167
1239.505718	46.047009	67.677172
1239.630547	44.486719	67.682177
1238.782227	52.235307	67.687182
1237.821882	61.698502	67.692186
1237.311827	48.006841	67.697191
1236.677294	60.472759	67.702196
1235.738186	40.260873	67.707201
1234.974262	46.037482	67.712206
1234.429908	52.709572	67.717210
1234.222905	51.701937	67.722215
1233.374776	47.431063	67.727220
1232.574255	41.716029	67.732225
1231.948503	43.391125	67.737230
1231.336617	43.901812	67.742234
1230.809786	48.224629	67.747239
1229.784618	49.348234	67.752244
1229.218491	46.260955	67.757249
1228.967682	50.877345	67.762254
1228.164475	47.411454	67.767258
1227.267559	44.578625	67.772263
1226.255404	48.964426	67.777268
1226.345199	45.908460	67.782273
1225.697245	45.306835	67.787278
1224.605998	50.511030	67.792282
1224.097341	43.456496	67.797287
1223.367467	52.296418	67.802292
1222.632619	40.780422	67.807297
1221.696829	49.165814	67.812302
1221.166463	43.401515	67.817306
1220.698531	47.197731	67.822311
1220.071465	52.184613	67.827316
1219.364608	47.881817	67.832321
1218.445964	46.440153	67.837326
1217.984102	43.531837	67.842330
1217.832309	45.082681	67.847335
1216.917432	50.347141	67.852340
1216.502048	39.639779	67.857345
1215.367082	47.340915	67.862350
1215.079563	41.284113	67.867354
1213.879949	34.747891	67.872359
1213.247316	52.556169	67.877364
1213.137200	41.801838	67.882369
1212.379737	50.376492	67.887374
1211.518557	38.188317	67.892378
1210.591453	42.204209	67.897383
1209.947082	50.543261	67.902388
1209.606944	40.543019	67.907393
1208.676066	46.577993	67.912398
1208.070377	40.954987	67.917402
1207.588500	40.530380	67.922407
1207.036942	46.501880	67.927412
1206.299847	35.424642	67.932417
1205.270905	43.160957	67.937422
1204.785232	44.164085	67.942426
1204.570902	42.547343	67.947431
1203.495751	45.930775	67.952436
1202.619180	37.931825	67.957441
1202.137237	51.272328	67.962446
1201.521079	41.099941	67.967450
1201.491399	43.000370	67.972455
1200.246197	53.647420	67.977460
1199.638670	41.567142	67.982465
1198.964397	46.320261	67.987470
1198.318225	33.914978	67.992474
1197.442719	44.807580	67.997479
1196.325334	44.703235	68.002484
1196.222384	42.947358	68.007489
1196.115421	40.455688	68.012494
1195.228072	47.617563	68.017498
1194.556047	35.361471	68.022503
1193.460231	43.520006	68.027508
1193.470391	35.886240	68.032513
1192.209549	48.025982	68.037518
1192.081114	37.162609	68.042522
1191.352555	39.926381	68.047527
1189.922334	45.305920	68.052532
1189.766232	39.176185	68.057537
1189.297744	43.355689	68.062542
1188.385562	39.864567	68.067546
1187.805085	41.423664	68.072551
1186.820719	38.231025	68.077556
1186.494220	36.783511	68.082561
1185.634719	40.273000	68.087566
1184.742023	41.383439	68.092570
1184.192610	36.806463	68.097575
1183.947496	37.875414	68.102580
1183.429187	36.997718	68.107585
1182.190337	49.422547	68.112590
1181.133928	39.548841	68.117594
1180.964579	37.391945	68.122599
1180.598228	53.582516	68.127604
1180.377011	42.626665	68.132609
1179.101714	40.901119	68.137614
1178.702051	35.679015	68.142618
1177.991922	47.191865	68.147623
1176.752471	43.867911	68.152628
1176.217123	37.240257	68.157633
1175.953692	46.871741	68.162638
1175.391572	44.247459	68.167642
1174.736434	36.300037	68.172647
1173.370285	48.360341	68.177652
1173.165190	43.980915	68.182657
1172.513860	40.197580	68.187662
1172.126865	37.501293	68.192666
1171.323774	41.800246	68.197671
1170.360360	41.127382	68.202676
1170.151911	43.076742	68.207681
1169.191046	45.989430	68.212686
1168.155157	41.740560	68.217690
1167.942665	47.960912	68.222695
1167.242684	47.280844	68.227700
1166.934067	43.599121	68.232705
1166.006860	46.366110	68.237710
1164.956791	42.567346	68.242714
1164.796563	45.832088	68.247719
1164.067814	46.004990	68.252724
1163.446428	39.676449	68.257729
1162.790201	51.437772	68.262734
1161.909227	46.785799	68.267738
1161.098124	42.244140	68.272743
1160.330066	53.050281	68.277748
1160.086652	45.411111	68.282753
1159.718152	45.730143	68.287758
1158.853439	41.258512	68.292762
1158.252834	41.278571	68.297767
1156.991133	48.389611	68.302772
1156.962832	43.256677	68.307777
1155.705537	49.285238	68.312782
1154.749883	48.794070	68.317786
1154.540297	53.741373	68.322791
1153.891482	44.422589	68.327796
1153.773161	40.600217	68.332801
1152.842125	43.106046	68.337806
1151.773112	42.757488	68.342810
1151.897389	37.576635	68.347815
1150.929946	44.453218	68.352820
1150.167005	33.958852	68.357825
1149.707223	44.979306	68.362830
1148.513118	40.255720	68.367834
1147.985505	35.088666	68.372839
1147.076548	40.759052	68.377844
1146.647409	33.247200	68.382849
1146.288839	42.122691	68.387854
1145.457097	42.348248	68.392858
1144.631214	39.281806	68.397863
1144.007404	44.194066	68.402868
1143.568927	45.889858	68.407873
1142.999536	42.711658	68.412878
1142.090687	45.169809	68.417882
1141.878030	46.124793	68.422887
1140.548528	45.281511	68.427892
1139.741825	49.754512	68.432897
1139.176032	44.866340	68.437902
1138.418048	49.885098	68.442906
1138.417339	41.988136	68.447911
1137.755996	49.908857	68.452916
1137.265682	46.532002	68.457921
1136.447265	47.097638	68.462926
1135.784927	51.582372	68.467930
1134.654020	45.462611	68.472935
1133.798698	53.023107	68.477940
1133.355515	44.549977	68.482945
1133.003780	44.978309	68.487950
1132.606314	43.447474	68.492954
1131.610982	46.938085	68.497959
1130.779805	43.344215	68.502964
1130.664674	40.295614	68.507969
1129.282939	45.031966	68.512974
1128.421054	48.957088	68.517978
1127.917579	35.213969	68.522983
1127.304568	49.899947	68.527988
1127.313534	35.398813	68.532993
1126.940800	39.788596	68.537998
1125.485855	38.414925	68.543002
1125.202187	44.779060	68.548007
1124.393903	42.490410	68.553012
1123.738329	32.478867	68.558017
1122.743060	40.306044	68.563022
1122.108215	39.787516	68.568026
1121.812773	41.698677	68.573031
1120.620829	49.557143	68.578036
1120.458317	39.632748	68.583041
1119.820364	46.316585	68.588046
1119.185645	40.669838	68.593050
1118.463076	41.138234	68.598055
1117.557496	41.985819	68.603060
1117.339064	40.598396	68.608065
1116.474414	39.532955	68.613070
1115.558082	49.257254	68.618074
1114.742070	45.135857	68.623079
1114.179290	46.370460	68.628084
1114.004556	42.587026	68.633089
1113.218588	40.657525	68.638094
1112.314172	45.370000	68.643098
1111.790941	36.873344	68.648103
1110.900451	49.614944	68.653108
1110.615792	43.896746	68.658113
1109.339475	36.644237	68.663118
1108.508615	38.351986	68.668122
1108.667762	31.695885	68.673127
1108.065291	42.310110	68.678132
1107.568128	40.799869	68.683137
1106.741143	40.368677	68.688142
1106.289394	41.292309	68.693146
1105.591439	29.966043	68.698151
1104.724973	40.436182	68.703156
1103.877585	36.255128	68.708161
1102.737232	46.086025	68.713166
1102.216719	39.720957	68.718170
1101.812019	34.420824	68.723175
1101.026223	50.301222	68.728180
1100.961685	40.629324	68.733185
1100.204779	48.049593	68.738190
1099.067026	36.643474	68.743194
1098.562689	35.522302	68.748199
1097.500918	44.042881	68.753204
1096.823439	34.588336	68.758209
1096.421698	40.933406	68.763214
1095.806706	42.108510	68.768218
1095.922815	34.364859	68.773223
1094.723246	40.488338	68.778228
1094.249312	36.063380	68.783233
1093.291912	41.962259	68.788238
1092.411709	46.111077	68.793242
1091.665518	37.987357	68.798247
1091.132462	40.161821	68.803252
1091.039705	34.233334	68.808257
1089.792080	47.580520	68.813262
1088.911983	42.930015	68.818266
1088.483984	40.784309	68.823271
1088.035947	39.272565	68.828276
1087.759681	36.394678	68.833281
1086.679478	46.955595	68.838286
1086.037195	43.095153	68.843290
1085.746409	43.643104	68.848295
1084.829619	51.893050	68.853300
1084.007377	40.766326	68.858305
1083.343229	40.325008	68.863310
1082.750241	36.737421	68.868314
1081.724183	36.542907	68.873319
1080.783583	39.414554	68.878324
1080.671364	33.258932	68.883329
1079.977843	38.947105	68.888334
1079.702517	39.625060	68.893338
1079.044385	44.344098	68.898343
1077.947264	42.863071	68.903348
1077.731289	47.757775	68.908353
1076.375940	51.717258	68.913358
1075.903516	40.148540	68.918362
1075.494647	40.045079	68.923367
1074.940982	40.097115	68.928372
1074.564009	34.403075	68.933377
1073.482347	46.091736	68.938382
1072.518703	44.949019	68.943386
1072.637485	39.321191	68.948391
1071.137222	44.934280	68.953396
1070.660582	43.496474	68.958401
1069.884816	47.541953	68.963406
1069.312938	43.641931	68.968410
1069.461544	38.648018	68.973415
1068.238468	47.296769	68.978420
1067.745058	38.461071	68.983425
1067.232442	35.196591	68.988430
1065.876311	42.355803	68.993434
1065.424507	47.283293	68.998439
1064.837335	48.006128	69.003444
1064.427822	43.354887	69.008449
1063.255061	47.670102	69.013454
1062.202831	45.242086	69.018458
1062.336326	44.555611	69.023463
1061.796005	52.955406	69.028468
1061.159289	38.979617	69.033473
1060.085456	47.014855	69.038478
1059.336123	47.017598	69.043482
1058.945478	38.572404	69.048487
1058.680930	51.469902	69.053492
1057.530606	45.392692	69.058497
1057.156666	52.515509	69.063502
1056.415399	50.227257	69.068506
1055.825450	47.165889	69.073511
1054.472407	43.625107	69.078516
1054.491673	43.242230	69.083521
1053.933733	38.754953	69.088526
1052.587961	48.993858	69.093530
1052.308739	42.035335	69.098535
1051.468872	47.385681	69.103540
1051.073114	43.008218	69.108545
1050.485041	48.905127	69.113550
1049.255809	42.987132	69.118554
1049.107222	43.678043	69.123559
1048.742196	50.331091	69.128564
1047.673986	41.944806	69.133569
1046.876205	46.727068	69.138574
1046.170370	47.803096	69.143578
1046.148581	42.132976	69.148583
1045.078818	37.987322	69.153588
1044.327742	46.945764	69.158593
1043.863886	46.094127	69.163598
1043.285699	37.057461	69.168602
1042.182197	48.156680	69.173607
1041.231665	47.912320	69.178612
1040.814551	40.644581	69.183617
1040.556411	40.788379	69.188622
1039.849109	56.519110	69.193626
1038.804612	43.887096	69.198631
1038.111247	44.705678	69.203636
1037.666968	43.321077	69.208641
1037.308500	40.703854	69.213646
1036.977514	44.120344	69.218650
1036.198844	39.852690	69.223655
1035.280632	46.421859	69.228660
1034.656180	42.533365	69.233665
1033.506765	47.149226	69.238670
1032.834870	43.339242	69.243674
1032.789191	41.057028	69.248679
1031.939457	45.440710	69.253684
1031.003578	43.533509	69.258689
1030.299583	49.374749	69.263694
1029.857807	47.951904	69.268698
1029.526354	42.197013	69.273703
1028.220147	46.091930	69.278708
1027.751126	47.576560	69.283713
1027.490208	35.870133	69.288718
1026.783187	49.418336	69.293722
1025.857144	41.947720	69.298727
1024.979288	40.718835	69.303732
1024.416275	39.767862	69.308737
1023.811411	36.609530	69.313742
1023.353039	44.269320	69.318746
1022.976259	42.213247	69.323751
1022.281397	45.422706	69.328756
1021.523770	50.256934	69.333761
1020.544606	49.039437	69.338766
1019.702883	48.210077	69.343770
1019.537175	43.319785	69.348775
1018.292547	55.580018	69.353780
1017.660588	37.183339	69.358785
1017.108560	49.349143	69.363790
1016.682898	47.099000	69.368794
1016.882846	36.658069	69.373799
1015.475721	51.263823	69.378804
1014.721251	51.991210	69.383809
1014.235750	47.563378	69.388814
1013.254994	50.075590	69.393818
1012.799618	46.439318	69.398823
1012.142443	53.906819	69.403828
1011.629857	47.819629	69.408833
1010.376565	47.317526	69.413838
1009.791938	47.637850	69.418842
1009.687061	50.256709	69.423847
1008.764129	44.439811	69.428852
1007.909627	49.464496	69.433857
1007.384042	49.477386	69.438862
1006.826098	46.527632	69.443866
1006.164804	37.378046	69.448871
1005.142296	39.483746	69.453876
1004.982383	37.599750	69.458881
1004.235548	44.177930	69.463886
1003.206450	48.861392	69.468890
1002.634286	42.105604	69.473895
1001.849057	48.691472	69.478900
1001.522862	43.121827	69.483905
1001.070697	49.534855	69.488910
1000.335111	41.576637	69.493914
999.651787	39.238186	69.498919
998.769542	49.865406	69.503924
998.255939	45.394741	69.508929
997.222554	41.787363	69.513934
996.509426	43.779187	69.518938
996.273161	40.615830	69.523943
995.518324	43.915262	69.528948
994.721821	34.842388	69.533953
994.135269	39.417590	69.538958
993.663019	42.257325	69.543962
993.119596	38.436375	69.548967
992.154887	41.620968	69.553972
991.683017	37.086898	69.558977
991.373889	38.498784	69.563982
990.103304	39.104873	69.568986
989.326678	37.716393	69.573991
988.768460	41.482852	69.578996
988.551694	35.408529	69.584001
987.438491	41.445770	69.589006
986.571619	38.182483	69.594010
986.163238	31.555184	69.599015
985.778223	50.798504	69.604020
985.492202	36.405829	69.609025
984.439698	38.394885	69.614030
983.839533	40.146390	69.619034
983.152217	42.742807	69.624039
982.056290	48.663765	69.629044
981.655730	38.871888	69.634049
981.108563	50.697882	69.639054
980.106464	48.774429	69.644058
979.643241	39.867722	69.649063
979.150496	43.511803	69.654068
978.774361	36.951912	69.659073
977.594744	44.100426	69.664078
976.576025	43.881132	69.669082
976.518923	42.228358	69.674087
975.794508	41.061807	69.679092
974.780796	40.086366	69.684097
973.975394	40.348789	69.689102
973.705007	39.436419	69.694106
973.387755	30.940150	69.699111
972.250115	39.534339	69.704116
971.520900	46.295802	69.709121
970.952922	38.350350	69.714126
970.319984	35.388887	69.719130
970.334406	30.570867	69.724135
969.215300	48.251558	69.729140
968.475908	40.752846	69.734145
968.046730	44.680124	69.739150
966.841643	41.672508	69.744154
966.281521	36.086480	69.749159
965.129501	44.900580	69.754164
964.872895	50.361565	69.759169
964.798764	38.627006	69.764174
963.900157	47.156360	69.769178
962.929547	32.986168	69.774183
962.244583	46.411019	69.779188
962.071395	39.348911	69.784193
961.632780	41.516256	69.789198
960.539096	44.298765	69.794202
959.869014	35.193172	69.799207
959.371643	41.622857	69.804212
958.353686	42.313341	69.809217
957.616227	35.069792	69.814222
957.035716	46.820667	69.819226
956.955714	34.087270	69.824231
955.951843	34.501127	69.829236
954.982376	34.772316	69.834241
954.520219	45.419427	69.839246
953.763294	34.288681	69.844250
953.571912	29.440334	69.849255
952.654224	42.241481	69.854260
952.142928	33.921169	69.859265
951.634154	35.396367	69.864270
950.184110	43.031041	69.869274
949.678354	43.655792	69.874279
949.239293	45.321746	69.879284
948.954177	35.246585	69.884289
948.204206	40.850730	69.889294
947.177900	42.561246	69.894298
946.664001	36.360748	69.899303
946.118020	46.598581	69.904308
945.332593	45.312439	69.909313
944.636672	46.391647	69.914318
943.672088	56.711869	69.919322
943.676757	43.775761	69.924327
942.015348	51.918735	69.929332
941.856007	46.188510	69.934337
941.293069	40.077816	69.939342
940.964722	49.126704	69.944346
940.604720	42.414442	69.949351
939.125080	48.047975	69.954356
938.754587	46.101301	69.959361
938.330826	40.105654	69.964366
937.255559	47.437849	69.969370
936.746670	38.653538	69.974375
935.988627	44.834553	69.979380
935.679186	41.961966	69.984385
934.447675	44.160876	69.989390
933.581469	43.493135	69.994394
933.302465	42.768220	69.999399
933.130747	45.908642	70.004404
932.862694	42.821314	70.009409
931.696640	39.298156	70.014414
930.888397	43.012952	70.019418
929.664999	34.222502	70.024423
929.121002	50.835564	70.029428
928.611093	44.880435	70.034433
928.201482	45.332196	70.039438
927.699667	45.059050	70.044442
927.330740	28.415116	70.049447
926.292608	39.620655	70.054452
925.439350	39.209473	70.059457
924.192277	47.805330	70.064462
923.680704	43.780635	70.069466
923.235876	37.608574	70.074471
922.546239	44.183978	70.079476
922.477239	36.468215	70.084481
921.958195	35.112881	70.089486
921.092528	31.892006	70.094490
920.555499	34.287903	70.099495
919.779064	36.922171	70.104500
918.893026	29.948285	70.109505
918.306560	36.122496	70.114510
917.572560	30.773887	70.119514
916.969835	36.848184	70.124519
915.670300	47.108173	70.129524
915.493965	38.720371	70.134529
914.999408	35.561862	70.139534
914.317789	38.712468	70.144538
913.404013	37.323762	70.149543
912.757268	46.410704	70.154548
912.076394	37.314730	70.159553
911.551069	39.968962	70.164558
911.174632	48.380538	70.169562
910.635930	36.667883	70.174567
909.741642	48.470277	70.179572
909.342644	37.257354	70.184577
908.349509	41.110389	70.189582
907.008755	41.576301	70.194586
907.165457	33.953930	70.199591
906.703997	46.879602	70.204596
905.739790	38.476841	70.209601
904.998685	34.717336	70.214606
904.222080	43.929022	70.219610
904.252721	40.507161	70.224615
903.157540	41.925884	70.229620
902.707265	46.583495	70.234625
901.851748	43.015661	70.239630
901.010910	38.862026	70.244634
900.530542	38.408855	70.249639
899.670568	39.758608	70.254644
899.060403	38.670091	70.259649
897.956822	44.220140	70.264654
897.190994	47.679041	70.269658
897.048707	45.878979	70.274663
896.717707	52.922434	70.279668
896.138439	38.439259	70.284673
895.233676	37.804476	70.289678
894.396957	44.791218	70.294682
894.120713	36.912901	70.299687
892.919419	50.796826	70.304692
892.347410	40.183869	70.309697
892.052086	48.234034	70.314702
891.536411	42.568412	70.319706
890.445147	38.825216	70.324711
889.590318	36.187669	70.329716
889.175272	37.012458	70.334721
888.623277	41.246293	70.339726
887.574342	39.579491	70.344730
887.120412	44.904727	70.349735
886.624627	46.239100	70.354740
886.122269	46.402859	70.359745
885.273595	50.559337	70.364750
884.633197	46.520461	70.369754
884.420192	42.426180	70.374759
882.998105	46.505188	70.379764
881.966458	45.920565	70.384769
881.737115	44.323593	70.389774
881.020208	39.967317	70.394778
881.225755	41.163263	70.399783
879.955523	45.262257	70.404788
879.096913	37.940248	70.409793
878.459814	39.459537	70.414798
878.173747	43.423973	70.419802
877.489176	37.102426	70.424807
876.340465	37.704944	70.429812
875.842973	39.211476	70.434817
875.601483	36.864242	70.439822
874.513086	40.721411	70.444826
873.949120	35.355215	70.449831
873.160715	44.160360	70.454836
873.018483	33.658782	70.459841
872.241138	37.464868	70.464846
871.096264	38.505165	70.469850
870.687041	40.486498	70.474855
869.804614	41.513410	70.479860
868.888495	37.944196	70.484865
868.339668	34.411141	70.489870
868.022124	42.814920	70.494874
867.843394	35.059859	70.499879
866.631365	43.298503	70.504884
865.858158	43.361873	70.509889
865.441361	38.912106	70.514894
865.076068	44.232699	70.519898
864.763527	39.501414	70.524903
863.653061	41.681091	70.529908
862.689911	39.562258	70.534913
861.767496	48.696239	70.539918
860.797859	39.113241	70.544922
860.464256	32.918764	70.549927
860.145708	49.054403	70.554932
859.547900	33.222766	70.559937
859.315894	42.519666	70.564942
858.143038	45.931398	70.569946
857.614396	35.376208	70.574951
857.003170	46.693594	70.579956
856.308954	39.072619	70.584961
855.479029	38.597825	70.589966
855.071378	38.888439	70.594970
854.228060	36.460382	70.599975
853.430953	41.310394	70.604980
852.871964	40.902861	70.609985
852.574297	35.319246	70.614990
850.897417	41.995029	70.619994
850.676124	37.556726	70.624999
850.114895	43.651241	70.630004
849.590265	35.722583	70.635009
849.167189	41.479722	70.640014
848.307937	45.937511	70.645018
847.849493	40.989758	70.650023
846.774089	37.242482	70.655028
845.846435	42.731433	70.660033
845.166476	37.088821	70.665038
844.594065	45.941594	70.670042
844.420672	33.858586	70.675047
843.948835	43.040698	70.680052
843.357231	42.029663	70.685057
842.308932	41.165437	70.690062
841.631179	34.680394	70.695066
841.276596	26.344637	70.700071
840.210593	41.817082	70.705076
839.719406	36.444042	70.710081
839.184519	38.552613	70.715086
838.098367	39.449539	70.720090
837.362720	36.636924	70.725095
836.710111	36.605414	70.730100
836.678885	34.167948	70.735105
835.623286	38.258027	70.740110
834.860357	31.673007	70.745114
834.685600	34.041218	70.750119
833.798029	32.088561	70.755124
832.783085	34.581047	70.760129
832.060028	33.756517	70.765134
831.408423	35.333319	70.770138
831.418040	34.070473	70.775143
830.836181	33.833741	70.780148
829.861518	39.620333	70.785153
829.220773	27.848264	70.790158
828.402540	37.112319	70.795162
827.187052	35.666017	70.800167
826.189638	33.309806	70.805172
826.090992	38.446033	70.810177
825.828781	41.048936	70.815182
825.703757	41.644646	70.820186
825.129112	29.278592	70.825191
823.982952	37.196109	70.830196
823.263599	31.447815	70.835201
822.372254	32.234891	70.840206
821.346155	36.922668	70.845210
821.187748	32.471205	70.850215
820.628029	30.281866	70.855220
820.076635	41.443074	70.860225
819.232676	37.225314	70.865230
818.265742	39.462586	70.870234
818.174264	41.784427	70.875239
817.172918	46.103997	70.880244
816.434623	43.766465	70.885249
815.956507	40.972786	70.890254
815.109117	42.610719	70.895258
814.753045	36.017710	70.900263
813.667426	49.383359	70.905268
813.559978	48.708418	70.910273
812.558365	39.885884	70.915278
811.186782	56.353153	70.920282
811.271287	36.193049	70.925287
810.530800	46.498128	70.930292
810.155519	43.068345	70.935297
809.079068	29.618400	70.940302
808.162666	43.169994	70.945306
807.827494	34.608803	70.950311
807.544106	35.355877	70.955316
806.803282	40.638483	70.960321
805.955822	38.761451	70.965326
805.417431	44.525913	70.970330
804.999126	38.318121	70.975335
803.561486	44.970043	70.980340
803.116633	38.820093	70.985345
802.470926	34.143433	70.990350
802.111127	40.048196	70.995354
801.711060	45.778025	71.000359
800.352192	43.763210	71.005364
800.137855	40.654735	71.010369
799.874252	29.991145	71.015374
798.403409	39.442673	71.020378
798.305755	36.309317	71.025383
797.229833	39.505373	71.030388
796.598877	28.591185	71.035393
796.070366	39.220480	71.040398
795.204737	39.632894	71.045402
795.345512	36.795892	71.050407
794.322591	36.359726	71.055412
793.092523	32.747483	71.060417
792.570794	28.795403	71.065422
792.187180	32.505715	71.070426
791.808972	26.173278	71.075431
790.695108	33.169469	71.080436
789.781750	34.879411	71.085441
789.261966	28.000240	71.090446
788.595087	40.671611	71.095450
787.883786	32.279111	71.100455
786.869022	45.524676	71.105460
786.914623	33.614973	71.110465
786.710448	34.918711	71.115470
785.964200	39.320680	71.120474
785.152591	37.086293	71.125479
784.363671	47.447972	71.130484
783.479173	40.721473	71.135489
782.739611	40.583973	71.140494
782.109176	46.285823	71.145498
781.784900	36.764128	71.150503
780.174380	40.619299	71.155508
779.818903	38.829533	71.160513
779.397579	37.316751	71.165518
778.480451	40.528536	71.170522
778.610655	40.706731	71.175527
777.573658	32.744547	71.180532
776.648387	42.134465	71.185537
776.328903	35.877833	71.190542
776.125849	36.124850	71.195546
775.075749	27.652254	71.200551
774.188528	45.535768	71.205556
773.725019	39.994336	71.210561
773.289749	35.541224	71.215566
772.021838	40.122437	71.220570
771.895561	39.601882	71.225575
771.064656	43.869103	71.230580
769.888313	39.505583	71.235585
769.718171	30.065012	71.240590
768.939840	35.022440	71.245594
768.675354	35.678201	71.250599
767.744290	31.073790	71.255604
767.146099	31.281213	71.260609
766.434103	39.561712	71.265614
765.271269	45.685787	71.270618
764.660494	23.576927	71.275623
764.016902	36.984169	71.280628
763.590769	34.800384	71.285633
763.337803	36.553432	71.290638
762.552704	43.170872	71.295642
761.847091	41.198735	71.300647
761.190240	40.731110	71.305652
760.496949	38.019009	71.310657
759.585361	34.266195	71.315662
758.907421	41.672387	71.320666
758.434887	30.111680	71.325671
757.663187	25.738943	71.330676
756.645136	35.656134	71.335681
756.307585	47.578081	71.340686
755.579736	48.452691	71.345690
755.670122	38.491253	71.350695
754.543074	38.109527	71.355700
753.967303	37.181148	71.360705
753.374383	33.200988	71.365710
751.894515	37.317645	71.370714
751.610881	27.494607	71.375719
750.630517	37.836303	71.380724
750.235617	39.673449	71.385729
750.141235	34.726107	71.390734
749.391679	33.323934	71.395738
748.659773	38.549940	71.400743
747.830305	39.618924	71.405748
747.231256	35.081507	71.410753
746.673914	35.932127	71.415758
745.469546	39.137615	71.420762
745.190086	37.220636	71.425767
744.757510	47.360012	71.430772
743.926021	42.878523	71.435777
743.223448	34.595034	71.440782
742.228750	38.946686	71.445786
741.961710	26.870730	71.450791
741.204058	40.275637	71.455796
740.655635	35.682854	71.460801
739.941355	32.806946	71.465806
739.405360	41.515163	71.470810
738.550450	36.739368	71.475815
737.311879	37.512371	71.480820
737.007197	30.592660	71.485825
737.041177	39.359937	71.490830
736.179768	34.569408	71.495834
735.416461	34.352126	71.500839
734.717466	47.895934	71.505844
734.224263	38.748069	71.510849
733.249117	30.872254	71.515854
732.390471	34.286050	71.520858
731.915014	34.093901	71.525863
731.576340	39.159534	71.530868
730.833668	47.252543	71.535873
730.235814	31.135546	71.540878
729.425622	40.234344	71.545882
728.508006	32.961219	71.550887
727.708451	42.020479	71.555892
727.381922	34.877167	71.560897
727.228976	31.588620	71.565902
725.742140	41.755502	71.570906
725.279214	34.965063	71.575911
724.365533	40.305171	71.580916
724.371587	34.548645	71.585921
723.601977	29.158467	71.590926
722.305970	40.569124	71.595930
721.940209	28.649237	71.600935
721.485324	41.816711	71.605940
721.343554	33.958020	71.610945
720.316329	31.008945	71.615950
719.390078	35.679283	71.620954
718.946953	38.452923	71.625959
717.622339	38.919520	71.630964
717.132510	42.050676	71.635969
716.642168	37.314612	71.640974
716.379875	46.539065	71.645978
715.893911	37.643940	71.650983
714.863657	44.287811	71.655988
714.406779	33.333318	71.660993
713.816298	28.392432	71.665998
712.417704	34.789023	71.671002
712.093076	30.999542	71.676007
711.470066	40.773428	71.681012
710.889931	34.999851	71.686017
709.911372	47.375517	71.691022
709.268466	47.779305	71.696026
708.813460	45.134931	71.701031
708.245355	43.386916	71.706036
707.959925	44.457597	71.711041
706.982134	39.643033	71.716046
706.486844	41.224938	71.721050
705.570902	40.300273	71.726055
704.747917	44.299750	71.731060
703.914236	39.807588	71.736065
703.453169	42.669242	71.741070
702.751749	47.781600	71.746074
702.238951	36.388165	71.751079
701.215241	36.978743	71.756084
701.188783	40.957047	71.761089
701.075135	37.461974	71.766094
699.548149	43.429594	71.771098
699.173259	42.965975	71.776103
698.547686	44.360472	71.781108
697.360988	38.735518	71.786113
696.503210	39.944642	71.791118
695.760041	54.020612	71.796122
695.582887	39.295293	71.801127
695.340532	49.249846	71.806132
694.433438	41.210246	71.811137
693.483311	45.269395	71.816142
692.733701	37.017067	71.821146
692.826326	34.722309	71.826151
691.710584	42.705996	71.831156
690.883500	36.987516	71.836161
690.422337	35.119977	71.841166
689.993422	41.210794	71.846170
689.127977	30.639908	71.851175
688.147913	46.768907	71.856180
687.994477	38.115726	71.861185
687.262641	36.325980	71.866190
686.093464	45.062490	71.871194
685.648989	32.756180	71.876199
685.293112	45.535738	71.881204
684.636028	39.194111	71.886209
683.995563	41.023061	71.891214
683.025455	39.651296	71.896218
682.633516	35.448344	71.901223
681.351871	36.806967	71.906228
680.383991	37.029124	71.911233
680.417765	39.908178	71.916238
679.725466	42.497578	71.921242
679.541533	36.842267	71.926247
678.574348	40.970367	71.931252
677.893555	43.431781	71.936257
677.625080	27.554093	71.941262
676.138717	40.297623	71.946266
675.716194	30.596062	71.951271
675.148051	41.468220	71.956276
674.911586	36.377931	71.961281
673.885145	31.541169	71.966286
672.938217	33.442575	71.971290
672.658203	30.125383	71.976295
671.951919	39.144570	71.981300
671.109183	40.037498	71.986305
670.489664	41.099882	71.991310
669.826485	49.043054	71.996314
669.813684	34.805654	72.001319
668.416226	42.640248	72.006324
667.612014	39.532682	72.011329
667.051620	44.887514	72.016334
666.610831	50.557611	72.021338
666.325838	36.279977	72.026343
665.191432	38.296394	72.031348
664.677268	31.662363	72.036353
664.318586	33.955793	72.041358
662.930653	39.792481	72.046362
662.548736	34.078816	72.051367
662.096022	40.550311	72.056372
661.393793	36.100312	72.061377
660.231708	34.427973	72.066382
659.638039	33.445699	72.071386
659.568700	24.611985	72.076391
658.835528	34.960072	72.081396
658.111517	32.669203	72.086401
657.171681	31.401438	72.091406
656.854212	44.135456	72.096410
656.319931	34.689811	72.101415
655.023213	38.272739	72.106420
654.278671	30.076393	72.111425
654.191868	34.125803	72.116430
653.704224	36.764618	72.121434
652.961769	37.764583	72.126439
652.085008	44.704149	72.131444
651.679064	33.459294	72.136449
650.567138	33.705979	72.141454
649.371627	38.370334	72.146458
649.409555	30.005230	72.151463
648.936520	35.229457	72.156468
648.596594	40.036680	72.161473
647.772203	38.048800	72.166478
647.073064	53.726231	72.171482
646.427907	39.474417	72.176487
645.340003	40.430050	72.181492
644.355751	39.921557	72.186497
644.155771	38.900245	72.191502
643.452007	44.326797	72.196506
642.295581	38.018973	72.201511
641.867797	36.453630	72.206516
641.342078	44.993069	72.211521
641.120013	37.930908	72.216526
640.541707	42.195785	72.221530
639.668039	40.865450	72.226535
639.044818	44.052554	72.231540
638.386432	40.027657	72.236545
637.391950	35.341937	72.241550
636.756196	43.954092	72.246554
636.628946	33.991055	72.251559
635.089533	42.606774	72.256564
634.287511	43.890616	72.261569
633.960986	50.671601	72.266574
633.467811	46.986241	72.271578
633.296923	29.071400	72.276583
632.442252	42.241045	72.281588
631.404238	41.851504	72.286593
630.964705	37.151524	72.291598
630.436797	36.724901	72.296602
629.812051	28.708180	72.301607
628.737488	45.456203	72.306612
627.998614	40.004391	72.311617
627.603081	37.788951	72.316622
627.148342	41.332418	72.321626
626.484781	35.360845	72.326631
625.613860	47.290465	72.331636
625.179037	39.186724	72.336641
624.207179	34.937370	72.341646
623.483330	38.856427	72.346650
623.265010	37.276651	72.351655
622.641390	41.182901	72.356660
621.786111	40.560838	72.361665
620.858983	41.410453	72.366670
620.160014	38.521106	72.371674
620.063541	31.330142	72.376679
618.863680	38.057824	72.381684
617.982817	35.500216	72.386689
617.947082	30.102008	72.391694
616.992802	37.566427	72.396698
616.331451	34.494475	72.401703
615.815621	45.482888	72.406708
615.211265	41.238084	72.411713
614.487942	32.089063	72.416718
613.192586	39.156803	72.421722
613.178690	41.407944	72.426727
612.646040	43.334856	72.431732
611.708035	42.243432	72.436737
611.060284	37.120886	72.441742
610.448497	44.169648	72.446746
609.914833	37.775274	72.451751
609.046064	34.261703	72.456756
608.181130	39.759661	72.461761
607.476423	33.321569	72.466766
607.189442	43.235915	72.471770
607.127712	30.324634	72.476775
605.892887	44.532526	72.481780
605.260029	42.809042	72.486785
605.259304	41.150459	72.491790
603.652409	41.464957	72.496794
603.324552	35.564502	72.501799
602.224428	35.815637	72.506804
601.946481	33.292897	72.511809
601.007768	37.091641	72.516814
600.352793	47.930333	72.521818
599.782169	34.649098	72.526823
599.168194	42.620711	72.531828
598.342810	33.957874	72.536833
597.834917	36.726078	72.541838
597.301448	44.922987	72.546842
596.596276	31.871340	72.551847
595.789881	37.659593	72.556852
595.107129	36.316214	72.561857
594.465090	31.301573	72.566862
594.130899	41.202937	72.571866
593.602858	35.026867	72.576871
592.644375	40.481383	72.581876
591.646433	37.849393	72.586881
591.899919	38.566175	72.591886
590.627847	39.068624	72.596890
590.001091	36.847441	72.601895
589.315684	42.040849	72.606900
588.817052	39.468104	72.611905
587.736639	38.419872	72.616910
587.067024	51.790291	72.621914
587.255439	38.776088	72.626919
586.394824	37.942003	72.631924
585.178526	39.173573	72.636929
584.641855	36.255234	72.641934
583.866536	41.964427	72.646938
582.857447	30.405658	72.651943
582.169819	36.548729	72.656948
581.779046	39.668860	72.661953
581.495554	28.335141	72.666958
580.422669	43.119633	72.671962
580.372725	40.757696	72.676967
579.750702	40.076419	72.681972
579.112346	36.997661	72.686977
578.218278	32.628707	72.691982
577.194871	35.423831	72.696986
576.337080	35.344647	72.701991
576.076032	39.385541	72.706996
575.580184	37.607128	72.712001
575.050273	33.142327	72.717006
573.934594	44.970595	72.722010
573.668350	37.147519	72.727015
573.219365	37.184569	72.732020
572.242952	46.577959	72.737025
571.475821	27.649525	72.742030
570.731646	39.347655	72.747034
570.549378	27.699777	72.752039
569.178989	33.096905	72.757044
568.499115	30.067342	72.762049
568.454637	26.832497	72.767054
567.330113	49.678584	72.772058
566.709383	36.023725	72.777063
566.209973	38.461006	72.782068
565.656527	37.628464	72.787073
565.172680	31.297132	72.792078
563.900173	42.715150	72.797082
563.786250	32.414118	72.802087
563.283521	32.491269	72.807092
562.173695	29.430845	72.812097
561.614249	27.842335	72.817102
560.673519	32.655376	72.822106
560.519644	31.066920	72.827111
559.167189	30.423148	72.832116
558.545778	38.835913	72.837121
558.490768	29.354963	72.842126
557.524215	37.543587	72.847130
557.359679	33.605632	72.852135
556.458710	36.210953	72.857140
555.779796	35.526129	72.862145
555.031658	32.384443	72.867150
554.074902	38.105195	72.872154
553.455905	36.726442	72.877159
552.965393	41.795776	72.882164
552.458902	36.529324	72.887169
551.317170	33.827218	72.892174
550.587935	41.564890	72.897178
550.413841	32.380447	72.902183
549.804473	43.582456	72.907188
549.308754	44.223034	72.912193
548.334759	42.810943	72.917198
547.313452	46.471479	72.922202
547.246314	34.399991	72.927207
546.640016	34.802720	72.932212
545.886154	46.579672	72.937217
545.388851	37.303211	72.942222
544.417498	40.569442	72.947226
543.936346	36.442228	72.952231
543.198123	41.819098	72.957236
542.543708	32.491974	72.962241
541.373843	29.362278	72.967246
540.584875	36.388809	72.972250
540.253610	35.888305	72.977255
539.909963	36.878391	72.982260
539.386755	36.044192	72.987265
538.676455	34.929141	72.992270
537.505630	38.239764	72.997274
537.330722	30.315419	73.002279
536.696374	36.276550	73.007284
535.548093	41.231471	73.012289
535.010920	35.675027	73.017294
534.655288	38.805335	73.022298
533.853639	34.263984	73.027303
532.754795	32.204749	73.032308
532.331602	32.847968	73.037313
532.253614	38.463438	73.042318
531.164314	39.233265	73.047322
530.652964	32.819593	73.052327
529.807446	41.736409	73.057332
529.012371	35.913549	73.062337
529.078959	35.895286	73.067342
527.613613	35.305784	73.072346
527.148807	43.510686	73.077351
526.809571	35.401208	73.082356
525.695333	34.547623	73.087361
525.177986	37.254268	73.092366
524.357221	38.323514	73.097370
524.282787	16.354847	73.102375
523.537855	27.127442	73.107380
522.609013	29.133251	73.112385
522.228141	38.483820	73.117390
521.215091	37.335002	73.122394
520.248466	31.235127	73.127399
519.643974	35.255042	73.132404
519.331935	36.541289	73.137409
519.174939	33.587715	73.142414
518.197296	36.802918	73.147418
517.356816	30.802797	73.152423
516.592633	32.561609	73.157428
516.133946	35.254181	73.162433
515.646412	29.850683	73.167438
514.573867	43.677946	73.172442
514.166182	34.480258	73.177447
512.974498	33.948093	73.182452
512.300481	36.045774	73.187457
512.010105	29.204252	73.192462
511.460592	37.555108	73.197466
511.102536	29.652059	73.202471
510.003006	36.314917	73.207476
509.166592	35.335080	73.212481
508.961612	31.096074	73.217486
507.994351	45.829069	73.222490
507.369162	33.187334	73.227495
506.603029	34.285728	73.232500
506.146999	35.471915	73.237505
505.845069	35.056627	73.242510
504.470762	36.289754	73.247514
503.982741	44.022125	73.252519
503.430042	38.748855	73.257524
502.693942	36.311730	73.262529
501.731668	36.157755	73.267534
501.119546	35.829730	73.272538
501.051570	36.167212	73.277543
500.554902	37.285758	73.282548
499.536689	42.975320	73.287553
499.163483	34.642607	73.292558
498.088171	39.294187	73.297562
497.188839	28.922751	73.302567
496.612071	30.560251	73.307572
495.768490	39.331689	73.312577
495.550268	34.221176	73.317582
495.077846	43.034410	73.322586
494.409358	36.890203	73.327591
493.621407	41.560660	73.332596
492.841706	39.903177	73.337601
492.234572	38.246589	73.342606
491.436891	44.112329	73.347610
490.597967	38.477815	73.352615
490.342977	42.224442	73.357620
489.783217	39.103227	73.362625
489.221930	38.297182	73.367630
488.256469	34.485254	73.372634
487.903593	31.162352	73.377639
486.508393	40.898442	73.382644
485.845898	35.604824	73.387649
485.460734	33.116527	73.392654
484.914345	50.463254	73.397658
484.832106	26.795899	73.402663
483.659902	37.840002	73.407668
482.809024	39.294098	73.412673
482.856181	23.052378	73.417678
481.625295	44.111418	73.422682
481.398788	35.558221	73.427687
480.506355	35.869360	73.432692
479.230312	39.059579	73.437697
478.672667	29.103640	73.442702
478.024186	27.300681	73.447706
477.771973	37.974294	73.452711
477.261789	25.173909	73.457716
476.556167	42.135995	73.462721
475.791853	24.714707	73.467726
475.134582	42.416552	73.472730
474.575648	34.441434	73.477735
473.363614	25.816603	73.482740
472.671712	28.186796	73.487745
472.448254	31.067398	73.492750
471.761136	31.128213	73.497754
471.013087	37.197357	73.502759
470.566959	21.097308	73.507764
469.625583	45.118998	73.512769
469.564615	29.930539	73.517774
468.117063	42.827252	73.522778
467.627393	31.061214	73.527783
467.292531	41.218150	73.532788
466.620760	42.727293	73.537793
465.977635	37.829556	73.542798
465.024239	41.886148	73.547802
464.852097	36.085489	73.552807
463.809265	35.097555	73.557812
462.614854	46.775980	73.562817
462.111134	32.902254	73.567822
461.887079	45.345425	73.572826
461.467614	33.282779	73.577831
460.456120	32.941124	73.582836
459.701600	36.579684	73.587841
459.812193	30.251443	73.592846
458.693444	37.079805	73.597850
457.828101	34.798902	73.602855
457.120869	30.925347	73.607860
456.526065	35.492500	73.612865
455.466404	31.744481	73.617870
454.621775	40.028826	73.622874
454.169857	25.389933	73.627879
453.817755	32.127687	73.632884
453.487439	35.447931	73.637889
453.029641	30.955904	73.642894
451.732592	38.012947	73.647898
451.587679	26.737605	73.652903
450.628054	30.523960	73.657908
449.602312	33.399928	73.662913
448.961337	32.767435	73.667918
448.551760	39.074388	73.672922
448.393527	28.260053	73.677927
447.672068	34.922619	73.682932
446.409341	33.204920	73.687937
446.178363	37.684147	73.692942
445.442611	31.501791	73.697946
444.499966	41.681450	73.702951
443.479069	43.452802	73.707956
443.317515	33.980956	73.712961
443.225072	30.752182	73.717966
441.814124	35.465144	73.722970
441.490709	28.373439	73.727975
440.901572	31.856344	73.732980
440.386442	29.234226	73.737985
439.553343	41.149971	73.742990
438.845359	38.564887	73.747994
438.215767	29.393118	73.752999
437.391354	31.868012	73.758004
436.701021	34.606966	73.763009
436.354684	31.447030	73.768014
435.005125	34.480252	73.773018
434.322246	33.341941	73.778023
433.592786	36.216438	73.783028
433.199473	38.908068	73.788033
433.027673	25.257436	73.793038
432.560634	34.874044	73.798042
431.516868	39.381853	73.803047
430.962296	33.705211	73.808052
430.229029	38.679202	73.813057
429.385817	36.427899	73.818062
428.509803	48.137605	73.823066
428.277688	29.731112	73.828071
427.764475	36.604925	73.833076
426.776740	37.631422	73.838081
426.307304	29.959024	73.843086
425.415468	38.552091	73.848090
424.920131	34.381436	73.853095
423.799315	43.550298	73.858100
423.224374	41.666251	73.863105
422.773625	34.049221	73.868110
422.232083	37.037279	73.873114
422.265736	33.837298	73.878119
421.021119	33.394035	73.883124
420.311424	38.480965	73.888129
419.241807	31.765201	73.893134
418.464042	40.160325	73.898138
418.070594	34.495859	73.903143
417.687806	38.567199	73.908148
417.156555	38.319347	73.913153
416.576220	27.395661	73.918158
415.615881	38.806568	73.923162
415.130033	33.874327	73.928167
413.690957	29.885591	73.933172
413.020797	42.920226	73.938177
412.933882	31.348646	73.943182
412.343828	37.644936	73.948186
412.275899	34.282950	73.953191
411.129005	35.055698	73.958196
410.416316	38.594568	73.963201
410.269480	36.468848	73.968206
408.887657	35.787262	73.973210
408.357096	32.082686	73.978215
407.867440	32.958863	73.983220
407.072649	40.136163	73.988225
406.102729	41.517792	73.993230
405.047267	36.945971	73.998234
404.851942	30.649131	74.003239
404.581569	40.696446	74.008244
403.488984	35.695311	74.013249
403.014946	33.888230	74.018254
402.274978	39.386834	74.023258
402.003393	38.952532	74.028263
401.277529	39.112579	74.033268
400.190030	37.538868	74.038273
399.856714	36.977210	74.043278
399.054622	30.639866	74.048282
398.592939	31.088971	74.053287
397.801946	36.291360	74.058292
397.078909	35.899035	74.063297
396.992437	32.300312	74.068302
395.692407	33.605239	74.073306
395.419543	31.431795	74.078311
394.407932	33.258456	74.083316
393.140987	34.999650	74.088321
392.852755	32.705655	74.093326
392.155542	48.682417	74.098330
392.095187	36.327603	74.103335
391.538955	30.950853	74.108340
390.226922	40.664273	74.113345
389.848992	31.332571	74.118350
389.254903	35.268854	74.123354
389.062271	29.857819	74.128359
387.871753	40.341915	74.133364
387.014027	39.540556	74.138369
386.997308	27.618758	74.143374
385.588897	39.246152	74.148378
385.092229	39.782835	74.153383
384.641895	29.270520	74.158388
383.745595	31.491962	74.163393
382.978796	27.282578	74.168398
382.144925	33.513648	74.173402
381.820853	37.499943	74.178407
381.254051	35.882688	74.183412
381.052568	31.576910	74.188417
380.245158	35.935112	74.193422
379.413067	35.798286	74.198426
378.859188	40.492972	74.203431
377.620020	34.874978	74.208436
376.824791	40.522741	74.213441
376.508604	27.653629	74.218446
375.842214	40.184627	74.223450
375.734815	38.741740	74.228455
374.904220	31.453332	74.233460
373.962147	37.821495	74.238465
373.733821	26.147883	74.243470
372.379714	34.567051	74.248474
371.823046	27.514109	74.253479
371.447760	37.669602	74.258484
370.517397	34.955979	74.263489
370.081648	28.296921	74.268494
369.138419	31.538231	74.273498
368.606837	28.390483	74.278503
368.229999	24.891652	74.283508
367.375899	33.574910	74.288513
366.695978	33.409108	74.293518
365.767811	33.579328	74.298522
365.622100	33.520778	74.303527
364.867297	33.470987	74.308532
363.842584	30.859133	74.313537
363.224186	36.071872	74.318542
362.551392	32.531898	74.323546
362.602072	31.850705	74.328551
361.578278	41.425165	74.333556
360.691762	40.147441	74.338561
360.842064	27.746453	74.343566
359.204138	32.706937	74.348570
358.748286	29.457238	74.353575
358.478220	33.018619	74.358580
357.311088	38.050732	74.363585
356.474025	37.041091	74.368590
355.960071	39.293073	74.373594
355.996985	33.593151	74.378599
354.933286	38.408512	74.383604
353.915545	26.581595	74.388609
353.606716	22.359161	74.393614
353.042531	34.208409	74.398618
351.854296	26.934432	74.403623
350.945803	36.878440	74.408628
350.559287	33.335422	74.413633
350.485756	31.120756	74.418638
349.939661	41.451705	74.423642
349.074079	29.516962	74.428647
348.202108	38.357613	74.433652
347.765882	34.997557	74.438657
347.240541	37.306547	74.443662
346.075852	44.946507	74.448666
345.452591	36.708874	74.453671
345.116274	35.975818	74.458676
343.874743	33.182488	74.463681
343.400880	31.433739	74.468686
343.051753	40.262028	74.473690
342.866002	34.384709	74.478695
341.343936	35.367089	74.483700
340.411045	42.963800	74.488705
340.324219	31.337026	74.493710
339.675930	32.728919	74.498714
339.193371	34.323054	74.503719
338.219222	29.310963	74.508724
337.567456	33.522948	74.513729
337.461744	28.339337	74.518734
336.000697	33.047722	74.523738
335.277546	29.641937	74.528743
335.018095	36.901088	74.533748
334.589489	29.450862	74.538753
334.450715	25.092521	74.543758
332.985590	40.956704	74.548762
332.544184	40.593629	74.553767
331.322351	35.233091	74.558772
330.444064	35.341759	74.563777
330.183325	26.089168	74.568782
329.540918	39.584579	74.573786
329.005068	33.289983	74.578791
329.162530	27.236546	74.583796
328.174862	28.037570	74.588801
327.567535	32.739204	74.593806
326.174048	35.020984	74.598810
325.391255	35.839819	74.603815
324.626610	28.878384	74.608820
323.982578	38.717174	74.613825
324.175416	30.787867	74.618830
323.367257	35.570396	74.623834
322.311591	26.146462	74.628839
321.861697	39.928153	74.633844
321.087689	36.098400	74.638849
320.594583	26.677845	74.643854
319.443410	32.666196	74.648858
319.006521	37.843707	74.653863
318.722810	40.030615	74.658868
317.941465	37.491954	74.663873
317.144304	30.594049	74.668878
316.439794	40.977057	74.673882
316.083580	38.481023	74.678887
315.432209	37.331416	74.683892
314.646599	44.978778	74.688897
314.415802	31.052147	74.693902
313.115746	41.008114	74.698906
312.559013	29.505125	74.703911
312.139969	39.702288	74.708916
311.194437	32.276110	74.713921
310.453227	35.501012	74.718926
309.556516	36.639201	74.723930
309.170245	31.678501	74.728935
308.831446	26.226121	74.733940
307.888524	29.659787	74.738945
307.316523	31.473183	74.743950
306.436918	39.977602	74.748954
306.275841	30.048398	74.753959
305.259847	34.616481	74.758964
304.242472	42.519976	74.763969
303.996157	37.355622	74.768974
303.336784	37.336370	74.773978
303.093215	31.707965	74.778983
301.890425	34.853478	74.783988
301.103595	38.312731	74.788993
301.099871	33.820904	74.793998
299.626014	32.680973	74.799002
298.848095	39.899765	74.804007
298.502752	34.549350	74.809012
297.975203	35.571933	74.814017
297.669837	37.386987	74.819022
296.695727	35.241750	74.824026
296.020459	28.575157	74.829031
295.635310	29.363736	74.834036
294.648793	26.337404	74.839041
293.940014	24.895762	74.844046
293.166858	27.411414	74.849050
292.969709	33.985713	74.854055
292.078437	27.063397	74.859060
291.063172	33.153097	74.864065
290.835273	21.058402	74.869070
289.922055	30.168984	74.874074
289.557380	38.137177	74.879079
288.883606	37.882109	74.884084
288.064366	31.456080	74.889089
287.615939	27.180215	74.894094
286.803137	38.102448	74.899098
285.957631	37.015332	74.904103
285.515524	30.562307	74.909108
284.743531	31.390472	74.914113
284.588680	29.308618	74.919118
283.183827	45.798719	74.924122
282.948404	31.579525	74.929127
282.220528	25.922668	74.934132
281.437103	31.786186	74.939137
280.731684	31.518819	74.944142
280.294503	37.331880	74.949146
279.844940	34.817617	74.954151
278.790646	39.849123	74.959156
277.540301	30.419973	74.964161
276.971595	34.826886	74.969166
276.893921	41.416836	74.974170
276.616333	28.305059	74.979175
276.073570	27.885612	74.984180
275.406634	30.918914	74.989185
274.744119	26.025910	74.994190
273.550420	37.948704	74.999194
273.022008	40.430083	75.004199
272.371594	35.689685	75.009204
271.125846	40.318059	75.014209
270.595249	27.656613	75.019214
269.833929	38.300990	75.024218
269.684169	42.075011	75.029223
269.460993	32.731287	75.034228
268.180222	33.831364	75.039233
267.901968	26.682036	75.044238
267.029198	36.306564	75.049242
266.460614	28.284169	75.054247
265.772899	23.474032	75.059252
264.899678	37.496662	75.064257
264.601197	36.382280	75.069262
263.571955	36.880880	75.074266
262.821076	34.228575	75.079271
262.313239	32.685527	75.084276
261.789352	33.303842	75.089281
261.257408	32.589367	75.094286
260.126429	32.151726	75.099290
259.704052	27.947408	75.104295
259.464552	33.514497	75.109300
258.171023	34.392690	75.114305
257.734415	35.755592	75.119310
256.762320	38.391276	75.124314
256.618887	32.600262	75.129319
256.042004	32.296643	75.134324
254.880604	41.085688	75.139329
254.583776	32.576861	75.144334
253.920277	33.026625	75.149338
252.972722	34.223400	75.154343
252.341194	26.870198	75.159348
251.504356	36.372309	75.164353
251.314299	33.526532	75.169358
250.613152	28.259655	75.174362
249.502457	28.001709	75.179367
249.167057	34.867700	75.184372
248.738730	37.270051	75.189377
247.968959	28.901273	75.194382
246.945199	44.679369	75.199386
246.404452	36.466463	75.204391
246.086394	31.840248	75.209396
244.976503	30.421562	75.214401
244.566319	28.744683	75.219406
243.804390	36.844012	75.224410
243.212570	35.867855	75.229415
242.440973	34.005743	75.234420
241.406001	34.831689	75.239425
241.495902	28.820560	75.244430
240.879871	28.844877	75.249434
240.462017	28.960602	75.254439
239.148202	33.776454	75.259444
238.261117	35.832478	75.264449
238.000719	26.344890	75.269454
237.250146	27.142847	75.274458
236.306989	29.240924	75.279463
236.001847	30.931371	75.284468
235.483241	37.246263	75.289473
234.575212	30.452796	75.294478
233.533131	34.756988	75.299482
233.128738	31.745112	75.304487
233.005785	29.431101	75.309492
231.995588	44.527387	75.314497
231.529569	45.040291	75.319502
230.853702	43.481459	75.324506
230.244125	36.263529	75.329511
229.252694	31.575934	75.334516
228.545601	33.033998	75.339521
228.296519	31.049171	75.344526
226.830645	32.580892	75.349530
226.030020	26.844191	75.354535
225.742199	35.558633	75.359540
225.247260	39.307259	75.364545
225.210963	33.712053	75.369550
224.410524	48.632983	75.374554
223.867423	33.049930	75.379559
222.931418	33.073224	75.384564
221.976263	36.273910	75.389569
221.177462	26.588313	75.394574
220.269067	24.191366	75.399578
220.158460	33.957744	75.404583
219.689486	40.242651	75.409588
218.491015	29.375001	75.414593
218.190445	29.123533	75.419598
217.474217	35.897277	75.424602
217.125801	30.607293	75.429607
215.764140	28.268415	75.434612
214.851198	38.971667	75.439617
214.814163	44.344062	75.444622
214.187096	37.895309	75.449626
213.714930	36.740815	75.454631
212.939695	39.423977	75.459636
212.251671	39.198010	75.464641
211.981445	38.528552	75.469646
210.415266	38.475700	75.474650
209.873670	35.469932	75.479655
209.610427	36.533974	75.484660
209.133861	39.609482	75.489665
208.272738	34.631467	75.494670
207.624043	32.694581	75.499674
207.051458	36.047166	75.504679
206.315589	36.983134	75.509684
205.266034	41.873567	75.514689
204.903798	25.575735	75.519694
203.967307	27.768953	75.524698
204.019073	32.737687	75.529703
202.994482	33.057380	75.534708
202.046363	41.814019	75.539713
201.598706	36.817396	75.544718
200.897061	37.629640	75.549722
200.057650	33.062898	75.554727
199.503287	32.236895	75.559732
199.004374	34.771930	75.564737
198.885283	31.575807	75.569742
197.565192	30.528116	75.574746
196.980761	30.976329	75.579751
196.416803	38.555262	75.584756
195.413127	38.039009	75.589761
194.836411	29.273628	75.594766
194.084074	29.423765	75.599770
193.873401	30.868925	75.604775
193.589424	24.018563	75.609780
192.291283	35.322537	75.614785
191.937322	37.304618	75.619790
191.038440	31.873748	75.624794
190.372411	36.641539	75.629799
189.786366	33.429979	75.634804
189.097804	37.893864	75.639809
188.545728	22.599267	75.644814
187.323122	38.886881	75.649818
186.836054	37.078770	75.654823
186.698931	30.460454	75.659828
185.638499	40.991691	75.664833
184.847274	30.007094	75.669838
183.974444	34.394704	75.674842
183.971974	31.705103	75.679847
183.452326	44.827733	75.684852
182.296708	35.973304	75.689857
181.852062	40.051379	75.694862
181.267461	43.323887	75.699866
180.759368	29.111926	75.704871
179.871617	37.691790	75.709876
178.579965	46.747634	75.714881
178.869714	44.243247	75.719886
178.141161	46.635132	75.724890
177.039979	43.961436	75.729895
176.371480	39.042606	75.734900
175.702173	41.507044	75.739905
175.354708	34.944341	75.744910
174.417916	39.140307	75.749914
173.952361	35.568927	75.754919
173.116494	39.425534	75.759924
172.036902	41.012391	75.764929
171.815933	28.582305	75.769934
171.020803	34.714218	75.774938
170.708267	33.072244	75.779943
170.096252	27.512069	75.784948
168.967366	33.697196	75.789953
169.019810	33.927179	75.794958
168.266173	36.269449	75.799962
167.007393	33.830618	75.804967
166.513805	32.173359	75.809972
165.513846	39.902237	75.814977
165.496928	20.966371	75.819982
164.417432	31.114303	75.824986
163.749118	32.164088	75.829991
163.389961	27.372559	75.834996
162.865853	28.919734	75.840001
162.221005	26.414558	75.845006
161.308616	31.915478	75.850010
160.341568	30.436211	75.855015
160.312999	40.227356	75.860020
159.234132	31.032706	75.865025
158.820156	31.814863	75.870030
157.957860	37.725683	75.875034
157.438999	28.894320	75.880039
156.610276	30.696643	75.885044
155.802115	39.487748	75.890049
155.643077	32.910775	75.895054
154.681956	42.197769	75.900058
154.137002	34.786638	75.905063
153.279564	32.151361	75.910068
152.541421	33.297437	75.915073
152.531904	25.294747	75.920078
151.117493	37.465660	75.925082
150.480403	30.673184	75.930087
150.030481	29.374811	75.935092
149.595069	38.078097	75.940097
149.019277	31.909768	75.945102
148.083463	37.368699	75.950106
147.667449	38.832412	75.955111
146.580459	43.333030	75.960116
145.615433	45.105054	75.965121
145.222138	34.298290	75.970126
144.685603	41.253130	75.975130
144.482528	43.606966	75.980135
143.692857	42.944650	75.985140
142.631483	50.505142	75.990145
142.479860	36.408232	75.995150
141.393493	42.488825	76.000154
140.701034	44.628965	76.005159
140.095923	32.510866	76.010164
139.331355	41.826446	76.015169
139.306339	43.779737	76.020174
138.049892	39.454553	76.025178
137.158017	42.416528	76.030183
137.045192	43.344631	76.035188
136.197434	40.972737	76.040193
135.644718	29.450248	76.045198
134.690740	35.512885	76.050202
134.186164	37.157875	76.055207
133.666632	41.788782	76.060212
132.539672	31.996277	76.065217
132.217364	29.310371	76.070222
131.707793	34.849569	76.075226
131.035583	32.214726	76.080231
130.199856	35.041595	76.085236
129.334594	43.267815	76.090241
129.011648	36.641288	76.095246
128.686278	43.527768	76.100250
128.017640	29.354042	76.105255
127.127625	35.750249	76.110260
126.269583	36.757760	76.115265
125.567151	22.151048	76.120270
124.482707	41.518450	76.125274
124.205783	37.741963	76.130279
124.175342	33.161367	76.135284
122.869404	35.170683	76.140289
122.019773	23.476358	76.145294
121.535140	28.183697	76.150298
121.301899	29.563076	76.155303
120.665164	22.453597	76.160308
119.129294	31.002786	76.165313
118.762327	33.311795	76.170318
118.343715	29.013868	76.175322
118.040138	34.895527	76.180327
117.116249	27.536953	76.185332
116.029860	29.047647	76.190337
116.075888	31.588836	76.195342
115.232722	39.680650	76.200346
114.164873	30.342345	76.205351
113.574004	28.807841	76.210356
112.929538	37.158121	76.215361
112.884434	33.891861	76.220366
111.582999	31.707439	76.225370
110.868847	37.438533	76.230375
110.614482	30.269656	76.235380
109.694357	34.505562	76.240385
109.226261	27.752383	76.245390
108.251751	38.161134	76.250394
107.857598	23.908959	76.255399
107.377923	32.250304	76.260404
106.671982	41.562850	76.265409
105.799094	28.374164	76.270414
105.246116	35.889859	76.275418
104.678200	35.301001	76.280423
103.973837	29.946380	76.285428
103.070098	35.247248	76.290433
102.838259	33.321186	76.295438
101.481892	29.671112	76.300442
100.729552	28.173399	76.305447
100.403797	36.977470	76.310452
99.984813	40.710850	76.315457
99.775750	36.254932	76.320462
98.366894	43.320505	76.325466
98.189416	37.739938	76.330471
97.373558	35.369280	76.335476
96.116456	43.711611	76.340481
96.129991	29.074306	76.345486
95.399287	34.189890	76.350490
94.597389	30.367821	76.355495
93.727742	34.524721	76.360500
93.013694	35.326358	76.365505
92.572338	32.415020	76.370510
92.268040	44.397895	76.375514
91.207672	38.762587	76.380519
90.666955	27.793277	76.385524
89.699657	34.857817	76.390529
89.519017	30.397370	76.395534
88.341610	31.222440	76.400538
87.821282	39.789467	76.405543
87.505398	32.455365	76.410548
86.734016	35.341371	76.415553
86.425914	29.745370	76.420558
85.216920	41.585520	76.425562
84.889780	34.103406	76.430567
84.065880	30.518234	76.435572
82.870979	33.333012	76.440577
82.623416	30.696694	76.445582
81.939678	37.302864	76.450586
81.599674	25.964089	76.455591
80.817673	36.384723	76.460596
79.680688	42.473412	76.465601
79.364455	36.927591	76.470606
78.975247	43.595601	76.475610
78.475898	30.268511	76.480615
78.022048	32.837379	76.485620
76.882394	49.152811	76.490625
75.963560	45.641123	76.495630
74.859398	46.320482	76.500634
74.786174	38.963449	76.505639
74.540541	32.196876	76.510644
73.279508	39.448614	76.515649
72.948478	41.594207	76.520654
72.384913	40.771279	76.525658
71.305172	32.768966	76.530663
70.748052	32.027010	76.535668
69.898057	34.922404	76.540673
69.873695	29.757384	76.545678
68.890090	35.944613	76.550682
67.816676	34.381424	76.555687
67.555828	27.330282	76.560692
66.804767	42.629700	76.565697
66.855261	38.378390	76.570702
65.808396	34.724706	76.575706
64.664677	37.689023	76.580711
64.565254	36.845689	76.585716
63.318037	38.060366	76.590721
62.845875	29.117508	76.595726
62.264562	36.811189	76.600730
61.222378	39.642623	76.605735
60.569346	30.626112	76.610740
59.882145	43.882702	76.615745
59.690860	32.256864	76.620750
59.193835	33.960587	76.625754
58.440337	28.440357	76.630759
57.587853	35.226406	76.635764
56.913657	43.553056	76.640769
56.808693	36.363512	76.645774
55.822883	42.350831	76.650778
55.289872	37.139202	76.655783
54.492828	39.857427	76.660788
53.129069	43.246342	76.665793
52.520825	31.579776	76.670798
51.912818	33.077278	76.675802
51.811519	35.091618	76.680807
51.479035	37.063984	76.685812
50.214160	40.637398	76.690817
49.386831	38.891469	76.695822
48.830288	42.332989	76.700826
48.651777	34.734140	76.705831
47.921363	36.120282	76.710836
46.919871	37.697890	76.715841
46.353619	41.115728	76.720846
45.879113	34.589084	76.725850
44.726226	34.498806	76.730855
44.288144	29.333543	76.735860
43.533967	38.491369	76.740865
43.467077	30.171415	76.745870
42.263728	37.740388	76.750874
41.963264	40.398338	76.755879
41.240653	33.706268	76.760884
40.373277	32.498152	76.765889
39.736777	28.089919	76.770894
38.870730	40.860959	76.775898
38.400985	33.306985	76.780903
37.913368	29.482119	76.785908
36.722559	39.023394	76.790913
36.140543	23.375673	76.795918
35.783076	27.618051	76.800922
34.995830	35.333543	76.805927
35.080160	32.647448	76.810932
33.974458	47.241789	76.815937
33.512624	30.185628	76.820942
32.500875	31.493646	76.825946
31.711665	31.154563	76.830951
31.363845	28.173128	76.835956
30.487777	41.462998	76.840961
29.810953	20.798461	76.845966
29.139926	36.827840	76.850970
28.407610	35.115650	76.855975
28.053007	32.592603	76.860980
27.336555	35.119788	76.865985
26.220823	33.055601	76.870990
25.834506	28.206931	76.875994
25.475779	39.316986	76.880999
25.038394	40.566513	76.886004
23.875368	41.368821	76.891009
23.434840	25.269613	76.896014
23.055332	27.320443	76.901018
21.936303	22.933988	76.906023
21.511237	25.200237	76.911028
20.171786	29.145094	76.916033
19.568102	20.634809	76.921038
18.826091	34.921979	76.926042
18.462454	32.608528	76.931047
18.035869	32.277839	76.936052
17.706492	25.985096	76.941057
16.939816	18.674035	76.946062
15.841266	25.119302	76.951066
15.519542	24.443890	76.956071
14.777434	21.709850	76.961076
13.645479	27.184337	76.966081
13.340365	17.325476	76.971086
12.710329	32.815317	76.976090
12.172110	24.703010	76.981095
11.177103	21.783811	76.986100
10.280507	28.286753	76.991105
10.190728	20.266920	76.996110
9.742261	27.325994	77.001114
8.956187	23.671742	77.006119
8.262448	30.036675	77.011124
7.504083	28.648761	77.016129
6.199161	21.045098	77.021134
5.646749	27.105219	77.026139
5.302883	25.610190	77.031143
4.870405	26.901514	77.036148
4.364403	33.919308	77.041153
3.788494	25.215364	77.046158